Mon Mar 08 18:04:22 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.461050	97.869071	0.000000
0.253923	94.243867	0.005005
-0.659251	61.846873	0.010010
-2.112475	7.235406	0.015014
-6.422655	-24.155959	0.020019
-11.321151	-14.196827	0.025024
-16.243388	-14.677755	0.030029
-20.999752	-18.025141	0.035034
-24.932408	-14.798896	0.040038
-28.939949	-10.955167	0.045043
-32.524309	-19.124008	0.050048
-36.459550	-13.915160	0.055053
-39.746968	-11.026774	0.060058
-43.595463	-11.626886	0.065062
-47.585082	-9.507968	0.070067
-50.750500	-14.168761	0.075072
-54.675105	-15.647667	0.080077
-58.598581	-14.974268	0.085082
-62.366792	-22.154972	0.090086
-66.062495	-12.527952	0.095091
-69.659918	-19.015245	0.100096
-73.793436	-11.354156	0.105101
-77.470231	-10.239123	0.110106
-81.208414	-21.567121	0.115110
-84.955016	-13.836857	0.120115
-88.585341	-24.942358	0.125120
-92.381095	-16.095679	0.130125
-96.151995	-12.814704	0.135130
-99.749601	-17.767591	0.140134
-103.726919	-3.454749	0.145139
-107.160128	-25.126981	0.150144
-111.546158	-11.225153	0.155149
-115.298809	-13.885689	0.160154
-118.467135	-15.340076	0.165158
-122.706096	-13.769441	0.170163
-126.111694	-23.731210	0.175168
-130.089461	-9.978065	0.180173
-134.015826	-18.686672	0.185178
-137.444826	-16.065718	0.190182
-141.472452	-14.624961	0.195187
-144.699766	-27.617574	0.200192
-148.671758	-16.848830	0.205197
-152.659767	-25.815639	0.210202
-156.373481	-25.541394	0.215206
-160.390379	-18.606806	0.220211
-164.186941	-18.877554	0.225216
-168.274365	-12.716996	0.230221
-171.975225	-20.199997	0.235226
-175.483919	-15.579373	0.240230
-179.481628	-1.241086	0.245235
-182.714038	-13.673040	0.250240
-186.959387	-2.942607	0.255245
-190.348011	-6.627759	0.260250
-193.646055	-11.227772	0.265254
-197.678901	-12.745940	0.270259
-201.464131	-11.364265	0.275264
-205.222240	-1.834311	0.280269
-209.196919	-5.061647	0.285274
-212.711995	-13.790027	0.290278
-216.891784	-13.813460	0.295283
-220.453200	-18.256288	0.300288
-224.474496	-12.708569	0.305293
-228.225718	-6.473837	0.310298
-231.437460	-21.395789	0.315302
-235.802986	-5.256242	0.320307
-239.273262	-21.896747	0.325312
-242.867817	-5.861311	0.330317
-246.238208	-17.793343	0.335322
-250.316764	-15.037025	0.340326
-254.280030	-5.259801	0.345331
-258.354765	-17.721200	0.350336
-262.086100	-9.480618	0.355341
-265.382560	-16.173331	0.360346
-269.067765	-18.659890	0.365350
-273.251781	-0.950269	0.370355
-276.873903	-11.619980	0.375360
-280.525148	-8.662164	0.380365
-284.467488	-9.579638	0.385370
-288.023353	-18.397578	0.390374
-292.017887	-14.675345	0.395379
-295.480666	-8.514939	0.400384
-299.234567	-8.603055	0.405389
-303.005809	-19.031303	0.410394
-306.873870	-21.122772	0.415398
-311.129759	-11.581020	0.420403
-314.640341	-22.930765	0.425408
-318.214341	-9.144021	0.430413
-322.131594	-14.463419	0.435418
-325.823541	-23.902949	0.440422
-329.510560	-7.553029	0.445427
-333.250492	-16.281594	0.450432
-336.856083	-12.684453	0.455437
-340.779079	-8.446874	0.460442
-344.134096	-14.072025	0.465446
-348.246888	-0.123530	0.470451
-352.300943	-11.247696	0.475456
-355.921621	-8.496491	0.480461
-359.624843	-14.092837	0.485466
-363.193013	-26.868288	0.490470
-367.173349	-10.512492	0.495475
-370.880874	-22.579734	0.500480
-374.593561	-15.636604	0.505485
-378.536598	-14.831834	0.510490
-382.523529	-17.175430	0.515494
-386.518588	-3.341865	0.520499
-389.750087	-21.573496	0.525504
-393.472672	-1.261361	0.530509
-396.822298	-19.105128	0.535514
-400.801691	-19.764190	0.540518
-404.996473	-18.509189	0.545523
-408.436236	-19.371088	0.550528
-412.336536	-14.383262	0.555533
-416.221919	-24.471402	0.560538
-419.566191	-14.007466	0.565542
-423.463671	-20.134067	0.570547
-427.234596	-14.518770	0.575552
-431.215543	-19.974462	0.580557
-435.072072	-11.682099	0.585562
-438.673687	-24.500972	0.590566
-442.576804	-13.861042	0.595571
-446.203816	-20.943817	0.600576
-449.835824	-14.180609	0.605581
-453.667386	-12.259726	0.610586
-457.021876	-14.234272	0.615590
-461.384966	-16.002020	0.620595
-464.896182	-12.843948	0.625600
-468.546192	-20.859693	0.630605
-472.533244	-20.025665	0.635610
-476.150327	-13.938138	0.640614
-480.210906	-9.079145	0.645619
-483.932369	-15.903936	0.650624
-487.610537	-20.835469	0.655629
-491.401506	-13.835510	0.660634
-495.028849	-10.985267	0.665638
-498.767071	-10.129435	0.670643
-502.171673	-12.732980	0.675648
-506.280681	-23.827579	0.680653
-510.327466	-16.395667	0.685658
-513.944590	-12.307585	0.690662
-517.999969	-8.624150	0.695667
-521.478770	-9.403960	0.700672
-525.288589	-15.165934	0.705677
-528.784889	-17.280147	0.710682
-532.562723	-18.553056	0.715686
-536.843991	-5.797881	0.720691
-540.195803	-10.986456	0.725696
-544.211915	-14.148258	0.730701
-547.603833	-3.551966	0.735706
-550.977081	-18.662100	0.740710
-555.036840	-11.462999	0.745715
-558.778278	-10.428369	0.750720
-562.741719	-15.434062	0.755725
-566.709194	-11.693627	0.760730
-570.301875	-14.096725	0.765734
-574.337435	-5.934816	0.770739
-577.583347	-13.505600	0.775744
-581.569757	-2.399576	0.780749
-585.400437	-1.981409	0.785754
-589.186318	-17.891286	0.790758
-592.843967	-10.193404	0.795763
-596.667498	-11.534602	0.800768
-600.444921	-4.282757	0.805773
-604.123441	-7.283929	0.810778
-607.805874	-21.319595	0.815782
-611.876786	-0.610913	0.820787
-615.446760	-23.266508	0.825792
-619.021151	-14.619984	0.830797
-622.988612	-10.706001	0.835802
-626.786526	-14.030247	0.840806
-630.570960	-9.483194	0.845811
-633.748358	-19.650950	0.850816
-637.728080	-18.477207	0.855821
-641.635823	-14.905460	0.860826
-645.778684	-14.383706	0.865830
-649.628715	-14.742907	0.870835
-653.142771	-14.151298	0.875840
-656.913686	-21.570276	0.880845
-660.567130	-12.422224	0.885850
-663.903293	-15.624649	0.890854
-667.836966	-3.337938	0.895859
-671.617333	-8.000548	0.900864
-675.750551	-12.058013	0.905869
-679.327127	-13.438534	0.910874
-682.914184	-18.343313	0.915878
-686.871401	-7.386868	0.920883
-690.820908	-6.705125	0.925888
-694.593431	-8.776533	0.930893
-698.266783	-13.052512	0.935898
-701.953100	-15.856745	0.940902
-705.980426	-8.992150	0.945907
-709.618311	-6.627162	0.950912
-713.117011	-14.578385	0.955917
-716.774515	-5.396484	0.960922
-720.704264	-10.028835	0.965926
-724.353690	-10.312742	0.970931
-728.210975	-10.749501	0.975936
-732.179581	-17.064475	0.980941
-736.117270	-13.833130	0.985946
-739.511802	-20.897393	0.990950
-743.026164	-6.313813	0.995955
-747.024154	-19.940858	1.000960
-751.195899	-4.671913	1.005965
-754.684218	-13.178222	1.010970
-758.231460	-16.551773	1.015974
-762.327166	-14.548763	1.020979
-765.750383	-7.627657	1.025984
-769.421906	-10.339535	1.030989
-773.392425	-9.362571	1.035994
-777.007712	-16.331577	1.040998
-781.072649	-7.511807	1.046003
-785.028453	-19.727896	1.051008
-788.902936	-15.743350	1.056013
-792.419076	-8.613398	1.061018
-795.602239	-12.464537	1.066022
-799.739159	-2.365406	1.071027
-803.537305	-8.341664	1.076032
-807.573531	-14.872771	1.081037
-811.227885	-10.015082	1.086042
-814.723298	-10.154738	1.091046
-818.441382	-7.327351	1.096051
-821.976578	-14.041016	1.101056
-825.862674	-7.845325	1.106061
-829.823325	-19.144383	1.111066
-833.330236	-18.176771	1.116070
-837.391128	-4.207421	1.121075
-841.042698	-15.696210	1.126080
-844.884380	-13.648511	1.131085
-848.910694	-6.343890	1.136090
-852.266186	-17.935179	1.141094
-856.200506	-12.945940	1.146099
-859.699604	-16.606142	1.151104
-863.787880	-13.572857	1.156109
-867.822336	-18.653397	1.161114
-871.030865	-20.256456	1.166118
-874.990846	-9.676155	1.171123
-878.628462	-16.250358	1.176128
-882.536295	-8.657130	1.181133
-886.359256	-6.219710	1.186138
-890.007906	-17.544885	1.191142
-894.103978	-6.097581	1.196147
-897.474438	-10.271859	1.201152
-901.239763	-7.840476	1.206157
-905.128364	-2.705506	1.211162
-908.676503	-17.859646	1.216166
-912.361388	-2.587858	1.221171
-916.366694	-12.879874	1.226176
-920.303786	-5.551555	1.231181
-923.855660	-13.176990	1.236186
-927.522798	-13.145525	1.241190
-931.322864	-17.714669	1.246195
-935.128674	-9.748179	1.251200
-938.902264	-21.149483	1.256205
-942.600339	-0.416344	1.261210
-946.647936	-17.143146	1.266214
-950.647943	-11.856257	1.271219
-953.521648	-7.735009	1.276224
-957.640749	-9.504577	1.281229
-961.386447	-12.138059	1.286234
-965.487493	-5.504091	1.291238
-969.446504	-13.865412	1.296243
-972.519860	-15.136722	1.301248
-976.720862	-10.162989	1.306253
-980.011603	-20.805679	1.311258
-983.464035	-25.338863	1.316262
-987.840297	-12.775900	1.321267
-991.295043	-29.329332	1.326272
-995.215565	-13.079931	1.331277
-999.244545	-13.988662	1.336282
-1003.046052	-22.848171	1.341286
-1007.010142	-2.212751	1.346291
-1010.544177	-17.310631	1.351296
-1014.070253	-10.178776	1.356301
-1018.208149	-7.287096	1.361306
-1021.300155	-12.630044	1.366310
-1025.636717	-4.591146	1.371315
-1029.076488	-22.750616	1.376320
-1032.747875	-9.199633	1.381325
-1036.911612	-11.323029	1.386330
-1040.516944	-26.814705	1.391334
-1044.433202	-4.955335	1.396339
-1048.030089	-14.632789	1.401344
-1051.828178	-10.587501	1.406349
-1055.857968	-11.174319	1.411354
-1059.364722	-19.205702	1.416358
-1063.020433	-9.787054	1.421363
-1066.888642	-15.800542	1.426368
-1070.693546	-12.749152	1.431373
-1074.070549	-13.246390	1.436378
-1077.764831	-12.975392	1.441382
-1082.324870	-6.991605	1.446387
-1085.767179	-5.541961	1.451392
-1089.071037	-4.155457	1.456397
-1092.879590	-12.832349	1.461402
-1096.650967	-11.870926	1.466406
-1100.832043	-10.091787	1.471411
-1104.244837	-18.478737	1.476416
-1108.147698	-12.694639	1.481421
-1111.780941	-7.149196	1.486426
-1115.403227	-33.879661	1.491430
-1119.446772	-10.527018	1.496435
-1123.094100	-16.031716	1.501440
-1127.071083	-6.675115	1.506445
-1131.197239	-1.309399	1.511450
-1134.754387	-15.044095	1.516454
-1138.474290	-0.034455	1.521459
-1142.000586	-9.049719	1.526464
-1145.610108	-14.815884	1.531469
-1149.424084	-2.921303	1.536474
-1153.045152	-7.917668	1.541478
-1157.339722	-11.549496	1.546483
-1160.800220	-3.767204	1.551488
-1164.789378	-17.986219	1.556493
-1168.494559	-6.884847	1.561498
-1171.860719	-13.722766	1.566502
-1175.613636	-11.553120	1.571507
-1179.534965	-8.506581	1.576512
-1183.495406	-5.669811	1.581517
-1187.313743	-7.332555	1.586522
-1191.217920	-13.890407	1.591526
-1194.924416	-5.696564	1.596531
-1198.315424	-13.978050	1.601536
-1201.773234	-12.200918	1.606541
-1205.935507	-8.021424	1.611546
-1209.647104	-19.433752	1.616550
-1213.577433	-8.433479	1.621555
-1217.127107	-12.886097	1.626560
-1221.014875	-18.547695	1.631565
-1224.827531	-5.167786	1.636570
-1228.614047	-15.398047	1.641574
-1232.348084	-10.038137	1.646579
-1236.415144	-13.491763	1.651584
-1239.952432	-15.036971	1.656589
-1244.003647	-17.781943	1.661594
-1247.195024	-18.639779	1.666598
-1250.933631	-6.730301	1.671603
-1254.778477	-11.334314	1.676608
-1258.542610	-17.591195	1.681613
-1262.455499	-2.695570	1.686618
-1265.801269	-14.677259	1.691622
-1269.872945	-10.695071	1.696627
-1273.846715	-16.159896	1.701632
-1277.717451	-10.875806	1.706637
-1281.405261	-12.500936	1.711642
-1284.555966	-17.569205	1.716646
-1288.691455	-13.286626	1.721651
-1292.518932	-18.106230	1.726656
-1296.333959	-13.635239	1.731661
-1300.194663	-13.975890	1.736666
-1303.515337	-21.082647	1.741670
-1307.661150	-14.797317	1.746675
-1311.301280	-16.773790	1.751680
-1314.646570	-16.537771	1.756685
-1318.703370	-19.292754	1.761690
-1322.321921	-18.207200	1.766694
-1326.466575	-12.726233	1.771699
-1330.386176	-12.395115	1.776704
-1334.012024	-5.816085	1.781709
-1337.816676	-21.213853	1.786714
-1341.149265	-16.034721	1.791718
-1344.927031	-21.981778	1.796723
-1348.846688	-12.170396	1.801728
-1352.565233	-11.440934	1.806733
-1356.597858	-14.901433	1.811738
-1359.972629	-9.480565	1.816742
-1364.048082	-15.764702	1.821747
-1367.400014	-27.622235	1.826752
-1371.300197	-20.712249	1.831757
-1375.383991	-19.869092	1.836762
-1379.193502	-13.817237	1.841766
-1383.099401	-14.700847	1.846771
-1386.980965	-24.313238	1.851776
-1390.347726	-18.836845	1.856781
-1394.074536	-17.063674	1.861786
-1397.241162	-19.189923	1.866790
-1401.716233	-13.651200	1.871795
-1405.528395	-15.721402	1.876800
-1408.836865	-21.237301	1.881805
-1412.867112	-21.873882	1.886810
-1416.231688	-22.285880	1.891814
-1420.530390	-16.810050	1.896819
-1423.859265	-18.747867	1.901824
-1427.454547	-17.883485	1.906829
-1431.784164	-14.793237	1.911834
-1435.183381	-22.688275	1.916838
-1439.271245	-20.986530	1.921843
-1443.125800	-21.460384	1.926848
-1446.751131	-10.664687	1.931853
-1450.880763	-11.916043	1.936858
-1453.943950	-20.348956	1.941862
-1457.862121	-13.634634	1.946867
-1461.576941	-17.224673	1.951872
-1465.491701	-23.815033	1.956877
-1469.426003	-12.753801	1.961882
-1472.878568	-22.056278	1.966886
-1476.972509	-15.326396	1.971891
-1480.691637	-13.945383	1.976896
-1484.275881	-21.222540	1.981901
-1487.932599	-8.404926	1.986906
-1491.346876	-15.422298	1.991910
-1495.295698	-9.045188	1.996915
-1499.550124	-22.310845	2.006912
-1500.729967	-18.032137	2.016909
-1498.281869	-12.163383	2.026906
-1495.033329	-15.190433	2.036902
-1492.793895	-20.097411	2.046899
-1491.138600	-14.207487	2.056896
-1489.731141	-10.962005	2.066893
-1487.277840	-13.860128	2.076890
-1485.320689	-11.618425	2.086886
-1483.336894	-15.647644	2.096883
-1481.739700	-13.956178	2.106880
-1479.781816	-10.258841	2.116877
-1478.005145	-11.665494	2.126874
-1475.875967	-13.234375	2.136870
-1473.884323	-5.819388	2.146867
-1472.081196	-11.911716	2.156864
-1470.223691	-14.002338	2.166861
-1468.521375	-8.353600	2.176858
-1466.493224	-11.069947	2.186854
-1464.384378	-16.805439	2.196851
-1462.604924	-19.660377	2.206848
-1460.705665	-13.035829	2.216845
-1458.925595	-9.445788	2.226842
-1457.176502	-12.401649	2.236838
-1455.124537	-16.860168	2.246835
-1453.150288	-14.207504	2.256832
-1451.500527	-11.289731	2.266829
-1449.786630	-19.148754	2.276826
-1447.731213	-17.704309	2.286822
-1445.578991	-19.336849	2.296819
-1443.842625	-16.106106	2.306816
-1441.749285	-14.794039	2.316813
-1440.210913	-9.539017	2.326810
-1437.998224	-13.783263	2.336806
-1436.450058	-6.265661	2.346803
-1434.532411	-17.160368	2.356800
-1432.394063	-16.891257	2.366797
-1430.567290	-15.313877	2.376794
-1428.959500	-15.262969	2.386790
-1427.301751	-16.660017	2.396787
-1425.075861	-17.440675	2.406784
-1422.914499	-17.726276	2.416781
-1421.333245	-8.952419	2.426778
-1419.379826	-4.340127	2.436774
-1417.398247	-18.012873	2.446771
-1415.501016	-21.863971	2.456768
-1413.687970	-19.796500	2.466765
-1411.950151	-7.136760	2.476762
-1410.010847	-13.768723	2.486758
-1408.113024	-19.561960	2.496755
-1406.245785	-20.346760	2.506752
-1404.215285	-20.210354	2.516749
-1402.590765	-14.566478	2.526746
-1400.568777	-13.612413	2.536742
-1398.813098	-14.346191	2.546739
-1396.827552	-16.496726	2.556736
-1395.019443	-15.053694	2.566733
-1393.156943	-8.358463	2.576730
-1391.203221	-19.353647	2.586726
-1389.135057	-12.625024	2.596723
-1387.289231	-21.911926	2.606720
-1385.629225	-14.931653	2.616717
-1383.819565	-13.157290	2.626714
-1381.937088	-9.698840	2.636710
-1380.058821	-21.725590	2.646707
-1378.065613	-19.208522	2.656704
-1376.211851	-19.579047	2.666701
-1374.133502	-23.034381	2.676698
-1372.068905	-14.121551	2.686694
-1370.537077	-19.548287	2.696691
-1368.874381	-23.606535	2.706688
-1366.785093	-20.321702	2.716685
-1364.792110	-19.574536	2.726682
-1363.128119	-21.826724	2.736678
-1360.957048	-25.448463	2.746675
-1359.380673	-15.386975	2.756672
-1357.542046	-17.967105	2.766669
-1355.586693	-22.064295	2.776666
-1353.522287	-17.262878	2.786662
-1351.658268	-24.097473	2.796659
-1349.881992	-19.688868	2.806656
-1348.115475	-22.366392	2.816653
-1346.298324	-25.026756	2.826650
-1344.115422	-16.911235	2.836646
-1342.278600	-21.284697	2.846643
-1340.623381	-14.658874	2.856640
-1338.440852	-13.132047	2.866637
-1336.587876	-18.720689	2.876634
-1334.976322	-18.875576	2.886630
-1333.231361	-22.664344	2.896627
-1331.147179	-21.693332	2.906624
-1329.135935	-20.961689	2.916621
-1327.183904	-23.002593	2.926618
-1325.636873	-22.621372	2.936614
-1323.538730	-24.346195	2.946611
-1321.763387	-17.913264	2.956608
-1319.760717	-17.353920	2.966605
-1317.744299	-14.439471	2.976602
-1316.156586	-17.069408	2.986598
-1314.115658	-17.105113	2.996595
-1312.412806	-18.757187	3.006592
-1310.502866	-17.518275	3.016589
-1308.655446	-14.060469	3.026586
-1306.767163	-12.800719	3.036582
-1304.828189	-18.883088	3.046579
-1302.987703	-16.971493	3.056576
-1300.824463	-20.535085	3.066573
-1299.216613	-11.940649	3.076570
-1297.529006	-14.543931	3.086566
-1295.370178	-7.626047	3.096563
-1293.555066	-15.774319	3.106560
-1291.622216	-11.049678	3.116557
-1289.644952	-16.328187	3.126554
-1287.854224	-9.329281	3.136550
-1286.130817	-11.131464	3.146547
-1284.272956	-11.982559	3.156544
-1282.263919	-14.065708	3.166541
-1280.599509	-11.628561	3.176538
-1278.503114	-20.518132	3.186534
-1276.624698	-17.014735	3.196531
-1274.611347	-18.138593	3.206528
-1272.957348	-10.735699	3.216525
-1271.203658	-16.690500	3.226522
-1269.196424	-14.505570	3.236518
-1267.193015	-16.221500	3.246515
-1265.236796	-19.483517	3.256512
-1263.425132	-13.217396	3.266509
-1261.872382	-19.083193	3.276506
-1260.071523	-13.427954	3.286502
-1257.737998	-20.463928	3.296499
-1255.816909	-4.386626	3.306496
-1254.152437	-8.817707	3.316493
-1252.231118	-5.188524	3.326490
-1250.606405	-4.134438	3.336486
-1248.465457	-6.661815	3.346483
-1246.547090	-6.957314	3.356480
-1244.875673	-5.883856	3.366477
-1243.050078	-9.309687	3.376474
-1240.898960	-12.427615	3.386470
-1238.952820	-10.761815	3.396467
-1237.414371	-7.903437	3.406464
-1235.444402	-10.577121	3.416461
-1233.394988	-3.190097	3.426458
-1231.702654	-3.078372	3.436454
-1229.508937	-3.422654	3.446451
-1227.951761	-11.703289	3.456448
-1225.993844	-8.076783	3.466445
-1224.195497	-8.796731	3.476442
-1222.309296	-17.066852	3.486438
-1220.418910	-9.700161	3.496435
-1218.365734	-7.637796	3.506432
-1216.576654	-11.214076	3.516429
-1214.659121	-8.283710	3.526426
-1213.082743	-13.690641	3.536422
-1211.108666	-7.382567	3.546419
-1208.978380	-13.451267	3.556416
-1207.176235	-17.116469	3.566413
-1205.471016	-11.613245	3.576410
-1203.326107	-14.097005	3.586406
-1201.749474	-13.579914	3.596403
-1199.591127	-15.604780	3.606400
-1197.908860	-11.736782	3.616397
-1195.881311	-10.510275	3.626394
-1194.100859	-2.963340	3.636390
-1192.198203	-14.758615	3.646387
-1190.139340	-9.640373	3.656384
-1188.621598	-19.599364	3.666381
-1186.651833	-14.705281	3.676378
-1184.765106	-8.290052	3.686374
-1182.972885	-12.239431	3.696371
-1180.926602	-9.773309	3.706368
-1179.069618	-9.362634	3.716365
-1177.360985	-14.545972	3.726362
-1175.281704	-7.078412	3.736358
-1173.333176	-11.138053	3.746355
-1171.445131	-5.195115	3.756352
-1169.653249	-1.028848	3.766349
-1168.084632	-8.449197	3.776346
-1165.829513	-3.818633	3.786342
-1163.959113	-0.230172	3.796339
-1162.042276	-5.997851	3.806336
-1160.613722	-7.113315	3.816333
-1158.521725	-1.419303	3.826330
-1156.525018	-0.048882	3.836326
-1154.873535	-1.089484	3.846323
-1152.420686	-9.143904	3.856320
-1150.844656	-6.741467	3.866317
-1149.251238	-6.268076	3.876314
-1147.197617	0.548374	3.886310
-1145.254311	-1.036263	3.896307
-1143.412655	-2.208331	3.906304
-1141.415701	-5.724657	3.916301
-1139.478238	-3.198457	3.926298
-1137.527517	-7.299473	3.936294
-1136.303839	-8.547933	3.946291
-1134.143258	-7.371073	3.956288
-1132.148168	-9.060296	3.966285
-1130.336946	-5.293398	3.976282
-1128.756821	-2.577397	3.986278
-1126.378098	-4.871130	3.996275
-1124.486770	-5.267990	4.006272
-1122.848434	-5.265966	4.016269
-1120.910367	-3.219835	4.026266
-1118.946598	-3.479862	4.036262
-1117.004474	-1.391745	4.046259
-1115.070397	-1.700702	4.056256
-1113.478939	-1.228553	4.066253
-1111.532956	-6.077194	4.076250
-1109.735602	-7.682664	4.086246
-1107.828594	-5.841548	4.096243
-1105.856341	-5.229785	4.106240
-1103.965513	-4.401316	4.116237
-1102.179847	4.548517	4.126234
-1100.375541	-0.067460	4.136230
-1098.354175	-6.598635	4.146227
-1096.595579	-6.528989	4.156224
-1094.717689	-4.184270	4.166221
-1092.584361	-5.767680	4.176218
-1090.898570	-1.399647	4.186214
-1089.160155	-10.852323	4.196211
-1086.836805	-12.290864	4.206208
-1085.359743	-13.627194	4.216205
-1083.404532	-15.939982	4.226202
-1081.521676	-8.620908	4.236198
-1079.414549	-6.769147	4.246195
-1077.879208	-8.430576	4.256192
-1075.676056	-11.668784	4.266189
-1073.896015	-10.667837	4.276186
-1072.185491	-11.668879	4.286182
-1070.314071	-7.510518	4.296179
-1068.389560	-16.640846	4.306176
-1066.469248	-8.381983	4.316173
-1064.507641	-5.299069	4.326170
-1062.793689	-16.183040	4.336166
-1060.897812	-13.481180	4.346163
-1059.114571	-13.349134	4.356160
-1057.269888	-17.194710	4.366157
-1055.468248	-8.255294	4.376154
-1053.121431	-13.799561	4.386150
-1051.487893	-3.896960	4.396147
-1049.522552	-2.456695	4.406144
-1047.482523	-11.621275	4.416141
-1046.027087	-3.900658	4.426138
-1044.134220	-7.237629	4.436134
-1042.038298	-4.545641	4.446131
-1040.061334	-10.727043	4.456128
-1038.218229	-17.862798	4.466125
-1036.282826	-13.463597	4.476122
-1034.547860	-14.110108	4.486118
-1033.010160	-14.856118	4.496115
-1030.955218	-18.141631	4.506112
-1029.011328	-13.006430	4.516109
-1027.155277	-17.542206	4.526106
-1025.016992	-15.138025	4.536102
-1023.281797	-14.676170	4.546099
-1021.428697	-14.612109	4.556096
-1019.674389	-17.401123	4.566093
-1017.668505	-15.604167	4.576090
-1016.072278	-16.828462	4.586086
-1013.985939	-8.673470	4.596083
-1011.908403	-15.205661	4.606080
-1009.905219	-11.571994	4.616077
-1008.585674	-12.145736	4.626074
-1006.619785	-14.182281	4.636070
-1004.571568	-13.952045	4.646067
-1002.734930	-15.386878	4.656064
-1000.757872	-9.792756	4.666061
-998.802692	-16.172741	4.676058
-997.015246	-14.978714	4.686054
-995.309926	-15.059943	4.696051
-993.176864	-16.133234	4.706048
-991.451136	-12.872014	4.716045
-989.559705	-16.456600	4.726042
-987.766997	-18.152812	4.736038
-985.769663	-11.178795	4.746035
-983.697365	-22.502113	4.756032
-982.156130	-15.455160	4.766029
-980.500508	-8.309655	4.776026
-978.265327	-8.657174	4.786022
-976.306039	-7.304298	4.796019
-974.388339	-2.725370	4.806016
-972.423071	-10.341659	4.816013
-970.536795	-10.568645	4.826010
-969.114703	-5.926253	4.836006
-967.139711	-13.498303	4.846003
-965.172231	-4.757426	4.856000
-963.353713	-13.284956	4.865997
-961.280378	-12.190298	4.875994
-959.557716	-7.288074	4.885990
-957.678967	-3.146578	4.895987
-956.198314	-10.075906	4.905984
-953.924704	-15.482060	4.915981
-951.889676	-18.399594	4.925978
-950.228926	-8.651263	4.935974
-948.260486	-9.513459	4.945971
-946.554628	-11.857317	4.955968
-944.318537	-9.009234	4.965965
-942.417101	-9.585982	4.975962
-940.610795	-6.443392	4.985958
-939.083333	-3.379371	4.995955
-937.046001	-9.425086	5.005952
-935.200965	-8.661788	5.015949
-933.259651	-4.715008	5.025946
-931.406017	-2.236804	5.035942
-929.664818	-8.923571	5.045939
-927.702708	-7.039012	5.055936
-925.383315	-7.747306	5.065933
-924.147502	-9.602321	5.075930
-922.177722	-9.436839	5.085926
-919.801861	-10.037316	5.095923
-918.028573	-8.907278	5.105920
-916.419025	-12.527266	5.115917
-914.656235	-11.300813	5.125914
-912.539191	-6.808966	5.135910
-910.859643	-13.762172	5.145907
-908.783921	-14.980953	5.155904
-907.085081	-15.659489	5.165901
-905.153957	-15.167293	5.175898
-903.431753	-8.409732	5.185894
-901.326264	-6.897012	5.195891
-899.376385	-7.806726	5.205888
-897.473141	-10.101582	5.215885
-895.633632	-13.529379	5.225882
-893.863862	-9.000943	5.235878
-892.015301	-10.180235	5.245875
-890.165612	-14.250693	5.255872
-888.041248	-12.898871	5.265869
-886.186345	-8.895606	5.275866
-884.485951	-16.357378	5.285862
-882.734487	-7.073482	5.295859
-880.825706	-11.268642	5.305856
-878.727004	-17.232542	5.315853
-877.127496	-18.326219	5.325850
-875.253677	-8.526627	5.335846
-873.226816	-11.818573	5.345843
-871.116801	-9.070261	5.355840
-869.432804	-14.603130	5.365837
-867.613699	-12.165145	5.375834
-865.702502	-12.342348	5.385830
-864.018014	-11.177547	5.395827
-862.122688	-4.337102	5.405824
-859.957958	-19.434496	5.415821
-858.181033	-11.547252	5.425818
-856.307620	-17.817744	5.435814
-854.343406	-21.066500	5.445811
-852.800236	-20.670137	5.455808
-850.562165	-14.645510	5.465805
-848.693298	-18.747423	5.475802
-847.182868	-23.644648	5.485798
-845.156756	-15.345660	5.495795
-843.316680	-16.040411	5.505792
-841.157513	-21.003440	5.515789
-839.453748	-10.658752	5.525786
-837.416396	-11.868180	5.535782
-835.582185	-10.840974	5.545779
-833.825290	-6.315167	5.555776
-831.965220	-17.497085	5.565773
-830.093376	-11.025484	5.575770
-828.305162	-8.604634	5.585766
-826.392571	-9.999370	5.595763
-824.582185	-12.975626	5.605760
-822.499685	-14.991188	5.615757
-820.465316	-8.825024	5.625754
-818.853121	-14.581641	5.635750
-816.989187	-12.948132	5.645747
-815.094856	-3.535437	5.655744
-813.022478	-9.540867	5.665741
-811.035220	-1.453517	5.675738
-809.356332	-10.268094	5.685734
-807.788389	-16.011316	5.695731
-805.672646	-6.843999	5.705728
-803.653549	-15.032434	5.715725
-801.787472	-15.085534	5.725722
-800.373065	-14.267512	5.735718
-798.396120	-9.819480	5.745715
-796.259322	-5.414362	5.755712
-794.431948	-12.694273	5.765709
-792.479014	-9.633420	5.775706
-790.428097	-7.020848	5.785702
-788.788131	-13.926598	5.795699
-787.015156	-11.994322	5.805696
-785.135182	-14.391159	5.815693
-783.042302	-14.035239	5.825690
-781.303544	-13.946398	5.835686
-779.416083	-17.774921	5.845683
-777.246325	-9.015675	5.855680
-775.502120	-14.613367	5.865677
-773.891817	-16.644997	5.875674
-772.107504	-12.008265	5.885670
-770.059229	-12.234139	5.895667
-768.089389	-14.653219	5.905664
-766.259555	-14.042092	5.915661
-764.310337	-9.588019	5.925658
-762.480416	-13.918903	5.935654
-760.691970	-12.855903	5.945651
-758.967236	-20.411481	5.955648
-756.700294	-10.368301	5.965645
-754.728924	-17.238573	5.975642
-753.610358	-15.075376	5.985638
-751.271991	-11.580306	5.995635
-749.377813	-13.903597	6.005632
-747.615542	-12.046947	6.015629
-745.851129	-10.953254	6.025626
-743.625314	-6.745466	6.035622
-741.827992	-5.274930	6.045619
-740.072436	-4.096134	6.055616
-737.944210	-8.462041	6.065613
-736.129803	-5.841623	6.075610
-734.416444	-5.448695	6.085606
-732.588076	-1.883156	6.095603
-730.675615	-14.360197	6.105600
-728.427085	-7.465555	6.115597
-726.753096	-12.107804	6.125594
-724.826890	-6.127945	6.135590
-723.279532	-8.474740	6.145587
-721.646871	-7.901542	6.155584
-719.646156	-7.027164	6.165581
-717.436027	-10.171429	6.175578
-715.342445	-5.524070	6.185574
-713.676316	-2.892572	6.195571
-711.913815	-6.754762	6.205568
-709.711881	-8.293533	6.215565
-708.056431	-6.500308	6.225562
-706.432574	-8.200909	6.235558
-704.364237	-4.187387	6.245555
-702.405397	-9.206710	6.255552
-700.595598	-7.403406	6.265549
-698.455722	-2.727113	6.275546
-696.975372	-5.857380	6.285542
-695.266642	-6.221562	6.295539
-693.274338	-5.438974	6.305536
-690.850792	-6.945245	6.315533
-689.506107	-5.096035	6.325530
-687.318594	-5.004620	6.335526
-685.486325	-5.102751	6.345523
-683.700290	-2.424075	6.355520
-681.974852	-8.252388	6.365517
-680.071133	-3.893600	6.375514
-677.975927	-3.226912	6.385510
-676.056091	-7.286317	6.395507
-674.342760	-10.526426	6.405504
-672.203610	-13.875620	6.415501
-670.333449	-11.082485	6.425498
-668.904197	-9.740975	6.435494
-667.131008	-8.054952	6.445491
-664.884172	-7.911416	6.455488
-662.832594	-11.759759	6.465485
-661.135449	-0.000727	6.475482
-659.321326	-6.313712	6.485478
-657.904979	0.079242	6.495475
-655.457617	-5.892818	6.505472
-653.465288	-9.106436	6.515469
-651.672383	-10.036657	6.525466
-650.059696	-8.419712	6.535462
-648.266606	-8.334717	6.545459
-645.927571	-11.496355	6.555456
-644.065427	-9.440850	6.565453
-642.759744	-13.863151	6.575450
-640.689595	-9.808810	6.585446
-638.826476	-7.890822	6.595443
-636.719994	-12.267378	6.605440
-634.919110	-7.792652	6.615437
-633.028131	-13.678956	6.625434
-630.945789	-4.597705	6.635430
-629.533810	-11.924821	6.645427
-627.515878	-10.465758	6.655424
-625.453414	-11.535338	6.665421
-623.450170	-9.764458	6.675418
-621.667707	-13.830295	6.685414
-619.848097	-9.244866	6.695411
-618.024315	-10.941033	6.705408
-616.486137	-14.566795	6.715405
-614.470948	-13.538328	6.725402
-612.172442	-7.014700	6.735398
-610.627176	-7.802700	6.745395
-608.601898	-10.899970	6.755392
-606.753328	-13.173234	6.765389
-604.965855	-9.784215	6.775386
-603.105758	-8.625174	6.785382
-601.236467	-10.333335	6.795379
-599.362778	-5.191275	6.805376
-597.370209	-13.572682	6.815373
-595.424252	-8.843210	6.825370
-593.547604	-12.955651	6.835366
-591.426905	-10.802462	6.845363
-590.085417	-17.223048	6.855360
-588.083870	-14.493465	6.865357
-586.167216	-9.246156	6.875354
-584.493246	-12.269919	6.885350
-582.336398	-9.544612	6.895347
-580.323334	-15.507220	6.905344
-578.694810	-12.028055	6.915341
-576.582633	-12.513440	6.925338
-575.054530	-9.922950	6.935334
-573.070105	-4.170148	6.945331
-570.903199	-7.817369	6.955328
-569.238813	-14.393733	6.965325
-567.386582	-12.781838	6.975322
-565.443429	-1.890953	6.985318
-563.771063	-6.976514	6.995315
-562.150581	-2.019762	7.005312
-559.590383	-9.583933	7.015309
-557.819356	-8.457997	7.025306
-556.337733	-14.735166	7.035302
-554.358465	-14.204584	7.045299
-552.274683	-9.042361	7.055296
-550.356117	-7.104737	7.065293
-548.491343	-11.834184	7.075290
-546.863768	-9.981129	7.085286
-544.927232	-6.969549	7.095283
-543.007500	-6.633129	7.105280
-540.927447	-13.920066	7.115277
-539.046560	-13.449546	7.125274
-537.448139	-12.577073	7.135270
-535.842974	-10.865691	7.145267
-533.904113	-8.673932	7.155264
-531.419058	-9.364093	7.165261
-529.705804	-12.015154	7.175258
-527.970054	-10.731985	7.185254
-526.116165	-10.730817	7.195251
-524.297537	-12.407143	7.205248
-522.608530	-10.038103	7.215245
-520.464728	-9.254303	7.225242
-518.429582	-7.995260	7.235238
-516.924820	-13.109283	7.245235
-514.775081	-11.372759	7.255232
-512.809713	-9.647839	7.265229
-511.060266	-9.162619	7.275226
-509.205229	-4.405918	7.285222
-507.579214	-12.916608	7.295219
-505.527038	-7.739820	7.305216
-503.478688	-12.648550	7.315213
-501.486683	-15.478317	7.325210
-499.865394	-8.102748	7.335206
-498.046447	0.104929	7.345203
-496.008033	-5.503251	7.355200
-494.157946	-10.077159	7.365197
-492.287824	-8.194907	7.375194
-490.442173	-5.966121	7.385190
-488.638036	-5.761192	7.395187
-486.728367	-2.390015	7.405184
-484.950213	-3.188285	7.415181
-482.919355	-4.390062	7.425178
-481.122836	2.614918	7.435174
-479.207512	-6.091959	7.445171
-477.255321	-9.321132	7.455168
-475.345166	-12.560957	7.465165
-473.467621	-12.931415	7.475162
-471.676902	-9.198605	7.485158
-469.654173	-8.799627	7.495155
-468.057914	-10.704081	7.505152
-466.014502	-18.264575	7.515149
-464.085058	-18.602261	7.525146
-462.190980	-13.125456	7.535142
-460.529590	-14.266635	7.545139
-458.477153	-15.705516	7.555136
-456.781042	-14.210706	7.565133
-454.878801	-11.130417	7.575130
-452.843650	-10.763408	7.585126
-451.208817	-7.042004	7.595123
-449.306685	-13.480999	7.605120
-447.379995	-15.398730	7.615117
-445.079905	-9.195704	7.625114
-443.512946	-12.838590	7.635110
-441.662863	-12.590438	7.645107
-439.863037	-1.141295	7.655104
-437.790483	-10.490605	7.665101
-435.973460	-12.753967	7.675098
-434.205206	-10.983296	7.685094
-432.615261	-14.920366	7.695091
-430.436467	-7.251666	7.705088
-428.440879	-7.672515	7.715085
-426.606946	-5.926535	7.725082
-424.757192	-7.265132	7.735078
-423.081362	-2.577638	7.745075
-420.942920	-10.788001	7.755072
-418.891881	-5.476743	7.765069
-417.218592	-12.766528	7.775066
-415.618907	-11.521549	7.785062
-413.520144	-9.710478	7.795059
-411.389724	-11.660711	7.805056
-409.594872	-10.432680	7.815053
-407.972008	-9.822964	7.825050
-405.950752	-11.814183	7.835046
-404.063492	-8.205679	7.845043
-402.418644	-7.683153	7.855040
-400.799723	-10.775371	7.865037
-398.506292	-7.943807	7.875034
-396.421753	-9.919859	7.885030
-394.642078	-2.553706	7.895027
-392.959300	-5.348227	7.905024
-391.197810	-3.476970	7.915021
-388.914667	-0.746382	7.925018
-387.264857	1.136394	7.935014
-385.295244	-4.307559	7.945011
-383.482160	-6.848146	7.955008
-381.691862	-4.267809	7.965005
-379.738719	-7.937577	7.975002
-377.649598	-2.903934	7.984998
-376.165016	0.500467	7.994995
-374.150689	-6.188490	8.004992
-372.200791	-5.997272	8.014989
-370.302354	-13.670337	8.024986
-368.646082	0.863316	8.034982
-366.716553	-1.083227	8.044979
-364.739315	-2.885809	8.054976
-362.868682	1.060117	8.064973
-360.861730	-5.185555	8.074970
-359.065621	1.334861	8.084966
-357.099361	-0.835430	8.094963
-355.309273	-3.519165	8.104960
-353.448979	-4.560975	8.114957
-351.487406	-1.954274	8.124954
-349.927175	1.400174	8.134950
-348.125806	1.406706	8.144947
-346.144588	-2.314887	8.154944
-343.778834	0.388347	8.164941
-342.144124	-5.884727	8.174938
-340.422923	-4.507518	8.184934
-338.634915	2.443676	8.194931
-336.343240	-1.439574	8.204928
-334.675765	-1.992701	8.214925
-332.798789	-2.089805	8.224922
-330.913947	1.888615	8.234918
-329.171531	-1.652741	8.244915
-327.347419	-2.532442	8.254912
-325.087424	-12.115268	8.264909
-323.442157	-10.710137	8.274906
-321.790277	-2.110911	8.284902
-320.035306	1.283522	8.294899
-317.764605	-1.007967	8.304896
-315.883367	-5.965661	8.314893
-313.916886	-1.345007	8.324890
-311.991238	0.138532	8.334886
-310.199200	1.578665	8.344883
-308.617626	-0.875965	8.354880
-306.682663	-9.704273	8.364877
-304.520769	-3.902192	8.374874
-303.001982	-0.727410	8.384870
-300.895018	-1.213301	8.394867
-298.803759	-3.630863	8.404864
-297.020485	-3.365619	8.414861
-295.463125	-4.490081	8.424858
-293.624142	-6.316326	8.434854
-291.421885	-2.415381	8.444851
-289.567639	-5.183519	8.454848
-287.740922	-0.575269	8.464845
-286.036961	-7.585666	8.474842
-284.335591	-3.271613	8.484838
-282.152215	-3.671790	8.494835
-280.213499	-2.861353	8.504832
-278.402215	-5.363682	8.514829
-276.359244	-13.872895	8.524826
-274.537035	-8.291302	8.534822
-272.826814	-7.337022	8.544819
-270.705105	-12.235171	8.554816
-269.104958	-5.269728	8.564813
-267.504967	-5.404676	8.574810
-265.337799	-7.832746	8.584807
-263.506087	-7.819942	8.594803
-261.558653	-11.202922	8.604800
-259.713652	-10.371196	8.614797
-257.609317	-9.495597	8.624794
-255.977129	-12.766680	8.634791
-254.017892	-10.528994	8.644787
-252.230825	-10.171166	8.654784
-250.122645	-11.254039	8.664781
-248.091942	-15.242394	8.674778
-246.740845	-9.966109	8.684775
-245.058452	-9.275785	8.694771
-242.576958	-13.358187	8.704768
-240.537933	-16.267881	8.714765
-238.700869	-15.240664	8.724762
-236.936151	-18.774461	8.734759
-235.257683	-13.174633	8.744755
-233.512720	-12.495866	8.754752
-231.536154	-21.266018	8.764749
-229.707034	-12.922379	8.774746
-227.616125	-16.762433	8.784743
-225.987916	-14.664523	8.794739
-224.131700	-14.095082	8.804736
-221.994190	-7.343257	8.814733
-220.273154	-9.447461	8.824730
-218.436181	-9.078626	8.834727
-216.502686	-11.202524	8.844723
-214.725121	-15.320978	8.854720
-212.860987	-10.538645	8.864717
-210.923075	-16.773181	8.874714
-209.064487	-10.875240	8.884711
-207.325814	-9.961769	8.894707
-205.160640	-11.540007	8.904704
-203.347729	-10.014706	8.914701
-201.278669	-13.279682	8.924698
-199.441153	-4.728934	8.934695
-197.736338	-10.061014	8.944691
-196.044601	-12.743149	8.954688
-194.077894	-15.546530	8.964685
-192.209598	-11.707461	8.974682
-189.960885	-17.852633	8.984679
-188.345125	-7.237573	8.994675
-186.880118	-12.668744	9.004672
-184.704619	-10.947082	9.014669
-182.910590	-11.098727	9.024666
-180.754566	-12.943901	9.034663
-179.048730	-7.168398	9.044659
-176.880796	-7.302336	9.054656
-175.423647	-6.776544	9.064653
-173.262708	-17.109213	9.074650
-171.371959	-11.205320	9.084647
-169.598449	-5.794288	9.094643
-167.728015	-9.578588	9.104640
-165.910767	-15.067532	9.114637
-164.109446	-13.587719	9.124634
-162.095528	-8.551353	9.134631
-160.049246	-8.264818	9.144627
-158.451039	-14.730897	9.154624
-156.512863	-15.230781	9.164621
-154.521725	-16.054900	9.174618
-152.776382	-14.318256	9.184615
-150.885671	-15.279503	9.194611
-149.093999	-13.614984	9.204608
-146.993526	-20.162774	9.214605
-145.246169	-10.263406	9.224602
-143.541109	-7.525604	9.234599
-141.304996	-8.061962	9.244595
-139.637884	-1.825518	9.254592
-137.624642	-6.254680	9.264589
-135.467571	-3.637938	9.274586
-133.874691	-11.412083	9.284583
-132.346841	-5.436043	9.294579
-130.369628	-7.956844	9.304576
-128.268267	-11.708487	9.314573
-126.703276	-10.280938	9.324570
-124.639715	-8.295048	9.334567
-122.381846	-8.118028	9.344563
-120.768363	-5.076654	9.354560
-119.217612	-8.980438	9.364557
-117.109516	-7.914266	9.374554
-115.075536	-6.362589	9.384551
-113.181828	-8.582690	9.394547
-111.513552	-2.336936	9.404544
-109.627092	-9.478969	9.414541
-107.752089	-6.596151	9.424538
-105.834341	-0.824399	9.434535
-104.110477	-6.129460	9.444531
-102.310688	-8.416672	9.454528
-100.197129	-10.297633	9.464525
-98.280595	-14.812384	9.474522
-96.454391	-2.907683	9.484519
-94.504984	-6.739266	9.494515
-92.691404	-1.445088	9.504512
-90.656747	-6.491832	9.514509
-88.848599	-8.870368	9.524506
-87.089858	-8.893156	9.534503
-85.191897	-5.879773	9.544499
-83.256764	-5.046501	9.554496
-81.456398	-2.855954	9.564493
-79.352221	-7.228526	9.574490
-77.790574	-12.146115	9.584487
-76.053763	-8.229134	9.594483
-73.950772	-2.065334	9.604480
-71.988795	-8.452029	9.614477
-70.141849	-13.888804	9.624474
-68.120895	-5.024581	9.634471
-66.435279	-8.195121	9.644467
-64.540208	-5.269680	9.654464
-62.778790	2.211764	9.664461
-60.789787	-12.896491	9.674458
-58.840569	-5.801844	9.684455
-57.168044	-11.095525	9.694451
-55.072128	-4.821634	9.704448
-52.983519	-4.642812	9.714445
-51.563148	-7.797872	9.724442
-49.754829	-8.390640	9.734439
-47.872863	-8.611476	9.744435
-45.588340	-19.759537	9.754432
-43.827218	-13.904333	9.764429
-42.084090	-12.727772	9.774426
-40.119934	-9.396496	9.784423
-38.503076	-1.323561	9.794419
-36.224468	-5.723923	9.804416
-34.422594	-6.070917	9.814413
-32.606527	-13.125878	9.824410
-30.584836	-18.031558	9.834407
-28.927719	-11.736599	9.844403
-27.100835	-10.464441	9.854400
-25.130574	-13.584042	9.864397
-23.030962	-8.444382	9.874394
-21.423066	-15.996648	9.884391
-19.504750	-9.171772	9.894387
-17.760408	-17.956837	9.904384
-15.635206	-12.046000	9.914381
-14.014648	-16.504005	9.924378
-11.877743	-20.850160	9.934375
-10.364247	-10.652856	9.944371
-8.059571	-10.753192	9.954368
-6.390561	-15.894702	9.964365
-4.609451	-18.613069	9.974362
-3.390805	5.385316	9.984359
-2.259155	50.482688	9.994355
-0.906572	117.646967	10.004352
0.000000	153.816708	10.009357
0.899057	200.587154	10.014362
1.177579	224.206395	10.019367
1.976071	257.474018	10.024371
2.794884	280.851059	10.029376
3.067422	302.482861	10.034381
3.272099	299.140427	10.039386
3.762523	324.880138	10.044391
3.765290	326.406393	10.049395
3.740119	340.771867	10.054400
4.111714	347.490530	10.059405
3.736980	350.821102	10.064410
4.182495	340.157904	10.069415
4.177290	346.391043	10.074419
4.233222	346.008599	10.079424
4.354743	349.468177	10.084429
4.019837	363.723803	10.089434
4.472584	358.078868	10.094439
4.458781	358.906028	10.099443
4.149936	368.082883	10.104448
4.762227	357.866157	10.109453
4.543180	383.354855	10.114458
4.532511	359.773485	10.119463
4.292641	361.516639	10.124467
4.233209	363.894909	10.129472
4.424883	370.426238	10.134477
4.338986	377.268347	10.139482
4.812356	369.869703	10.144487
4.609728	374.167885	10.149491
4.627973	375.590752	10.154496
4.556579	375.201808	10.159501
4.397605	390.774539	10.164506
4.582541	379.252435	10.169511
4.626951	396.327106	10.174515
4.866926	403.405833	10.179520
5.077524	408.300438	10.184525
5.243218	407.503094	10.189530
5.601565	415.868665	10.194535
5.506292	396.362965	10.199539
5.133865	393.735453	10.204544
5.468527	381.460914	10.209549
5.323438	387.052484	10.214554
5.504691	383.571843	10.219559
5.467337	389.360696	10.224563
5.469833	397.442392	10.229568
5.655575	395.761911	10.234573
5.502274	397.820845	10.239578
5.258649	395.420371	10.244583
5.365952	392.161256	10.249587
5.123063	404.621868	10.254592
5.687390	415.474558	10.259597
5.887198	433.032266	10.264602
5.885549	426.504144	10.269607
5.929383	423.562652	10.274611
5.831128	435.609137	10.279616
5.844657	435.575654	10.284621
5.897403	443.707708	10.289626
6.226120	426.927135	10.294631
5.945420	434.003768	10.299635
6.050828	437.301933	10.304640
5.985530	436.279655	10.309645
5.931195	430.933190	10.314650
6.050317	438.029633	10.319655
6.069292	444.490770	10.324659
6.175978	443.396906	10.329664
6.477236	438.728584	10.334669
5.951931	452.686659	10.339674
6.389191	441.024913	10.344679
6.345334	437.006150	10.349683
6.076093	452.525571	10.354688
6.399132	454.178954	10.359693
6.405883	475.474937	10.364698
6.920079	472.586148	10.369703
6.939847	476.617075	10.374707
6.800090	485.186713	10.379712
6.990007	478.411970	10.384717
6.962041	461.376008	10.389722
6.823366	462.161588	10.394727
6.919662	460.835990	10.399731
6.757196	462.033798	10.404736
6.975606	482.130658	10.409741
7.072079	476.850010	10.414746
7.020689	485.474940	10.419751
7.168916	495.170334	10.424755
7.126297	496.648653	10.429760
7.455472	485.322657	10.434765
6.980427	504.224426	10.439770
7.185880	489.885658	10.444775
7.394882	495.975885	10.449779
7.456390	495.748668	10.454784
7.310614	506.063399	10.459789
7.331415	492.555177	10.464794
7.703838	501.721228	10.469799
7.837734	501.181265	10.474803
7.467818	509.484849	10.479808
7.739648	499.027435	10.484813
7.701910	501.712930	10.489818
7.560984	504.679813	10.494823
7.798702	499.211048	10.499827
7.684882	513.948803	10.504832
7.647143	506.803500	10.509837
7.412209	505.975431	10.514842
7.626941	510.755870	10.519847
8.069687	500.621280	10.524851
7.729785	508.915346	10.529856
8.038363	514.052982	10.534861
8.003861	537.640658	10.539866
8.156286	533.604755	10.544871
8.590746	538.484200	10.549875
8.466574	539.414129	10.554880
8.559457	534.659163	10.559885
8.360354	543.438575	10.564890
8.316614	539.241568	10.569895
8.369902	534.265834	10.574899
7.872322	544.297656	10.579904
8.349522	538.487901	10.584909
8.045724	542.461644	10.589914
8.201897	554.866620	10.594919
8.274895	550.747185	10.599923
8.276563	564.998212	10.604928
8.726571	565.983222	10.609933
8.751773	583.900127	10.614938
8.813437	574.835529	10.619943
8.667722	578.913380	10.624947
8.877255	582.972418	10.629952
9.328607	581.924498	10.634957
9.310748	581.523855	10.639962
9.179044	584.033538	10.644967
9.059275	585.662944	10.649971
9.082910	585.063293	10.654976
9.298172	581.673375	10.659981
9.102160	590.684138	10.664986
9.272253	579.541139	10.669991
9.208156	584.069603	10.674995
9.047218	597.693731	10.680000
9.132774	595.437841	10.685005
9.390928	590.960853	10.690010
9.304497	586.316472	10.695015
9.284499	597.759245	10.700019
9.051406	597.823444	10.705024
9.715837	614.323236	10.710029
9.720490	625.281120	10.715034
9.660836	627.990634	10.720039
9.893738	632.282506	10.725043
9.806365	625.380031	10.730048
9.946252	625.597634	10.735053
10.024243	631.119024	10.740058
10.041977	625.943922	10.745063
10.220324	617.043617	10.750067
9.903221	603.075092	10.755072
10.158727	617.358226	10.760077
9.917064	625.488453	10.765082
10.198711	617.368047	10.770087
10.385452	621.556889	10.775091
10.043281	628.364295	10.780096
10.054149	632.363569	10.785101
9.873538	634.012146	10.790106
10.193070	632.390726	10.795111
10.470355	629.651659	10.800115
9.983524	630.759287	10.805120
10.388643	629.720314	10.810125
10.084912	636.042191	10.815130
10.031654	641.351126	10.820135
10.677360	653.048893	10.825139
10.383454	671.518282	10.830144
10.715103	666.286790	10.835149
10.570642	674.604972	10.840154
10.661905	673.535628	10.845159
11.026757	674.526344	10.850163
10.915272	667.288643	10.855168
11.304085	668.841673	10.860173
10.907636	680.465980	10.865178
10.612120	670.652453	10.870183
11.051159	664.919699	10.875187
10.944202	671.713265	10.880192
11.130399	676.726972	10.885197
10.827169	679.830166	10.890202
11.294997	671.031895	10.895207
11.138707	666.550021	10.900211
10.864193	690.045336	10.905216
11.407186	695.164573	10.910221
11.482614	704.570514	10.915226
11.655950	709.409662	10.920231
11.701199	710.471856	10.925235
11.395166	715.362231	10.930240
11.778382	713.107735	10.935245
11.793723	712.786950	10.940250
11.730611	707.217851	10.945255
11.527368	714.890983	10.950259
11.389697	721.522309	10.955264
11.800375	703.465178	10.960269
11.648275	711.067071	10.965274
11.869222	713.815427	10.970279
11.948813	711.998873	10.975283
12.036953	719.349560	10.980288
12.109458	704.921396	10.985293
11.791100	711.280332	10.990298
11.885020	713.560082	10.995303
11.992394	715.117004	11.000307
11.896305	718.959892	11.005312
12.055044	718.881170	11.010317
12.119710	731.076960	11.015322
12.237410	751.396843	11.020327
12.267222	747.583868	11.025331
12.245999	758.424552	11.030336
12.596469	743.116210	11.035341
12.614175	747.814609	11.040346
12.454551	755.755201	11.045351
12.289684	749.519477	11.050355
12.183392	758.990708	11.055360
12.742797	750.311828	11.060365
12.454628	753.937773	11.065370
12.262260	761.106134	11.070375
12.487083	766.585233	11.075379
12.760800	782.776941	11.080384
12.606746	794.567687	11.085389
12.758683	792.507766	11.090394
12.773168	787.339433	11.095399
12.959341	789.937227	11.100403
12.788964	787.133909	11.105408
13.379965	789.572516	11.110413
13.263526	793.524328	11.115418
12.891051	787.249159	11.120423
13.007863	800.315076	11.125427
13.052039	791.942281	11.130432
13.231701	810.549208	11.135437
12.779738	815.339885	11.140442
13.369837	820.374381	11.145447
13.253793	821.269914	11.150451
13.165161	829.789021	11.155456
13.211748	817.763495	11.160461
13.406871	836.294660	11.165466
13.354643	824.064897	11.170471
13.670958	846.992344	11.175475
13.839517	856.616927	11.180480
14.243831	854.359045	11.185485
14.003092	848.789836	11.190490
13.905256	827.012294	11.195495
14.114998	820.937572	11.200499
13.469943	840.555252	11.205504
13.716382	839.093706	11.210509
13.993251	855.430077	11.215514
14.123721	861.320088	11.220519
14.051588	858.357579	11.225523
13.870278	870.887617	11.230528
14.132869	868.303819	11.235533
13.934853	870.508727	11.240538
13.982591	867.799919	11.245543
14.275381	869.846120	11.250547
13.914232	867.295570	11.255552
14.474949	876.302514	11.260557
14.523485	888.362232	11.265562
14.265004	890.010641	11.270567
14.719016	902.164977	11.275571
14.678449	893.157489	11.280576
14.623243	895.270235	11.285581
14.402458	898.790848	11.290586
14.530582	889.803767	11.295591
14.634019	897.328729	11.300595
14.698197	893.060789	11.305600
15.022540	895.228121	11.310605
15.113139	889.025712	11.315610
14.983887	895.184249	11.320615
15.269717	889.344954	11.325619
15.028477	906.651871	11.330624
15.261270	897.605513	11.335629
14.804684	899.558341	11.340634
15.040665	895.512166	11.345639
15.009750	902.602804	11.350643
14.955894	894.065806	11.355648
15.080867	902.142442	11.360653
15.359270	905.097721	11.365658
15.730394	923.641141	11.370663
15.612387	922.592540	11.375667
15.039184	916.898128	11.380672
15.376493	932.602027	11.385677
15.241324	926.834594	11.390682
15.230751	939.971419	11.395687
15.525081	937.229576	11.400691
15.571339	940.450555	11.405696
15.487780	941.280988	11.410701
15.645668	937.583160	11.415706
15.493796	942.374903	11.420711
15.966958	955.015103	11.425715
15.748408	966.207548	11.430720
16.393882	961.096216	11.435725
15.976127	958.280278	11.440730
15.901623	962.594468	11.445735
16.197483	964.909862	11.450739
15.720551	970.649203	11.455744
15.846385	972.505995	11.460749
16.020698	968.501176	11.465754
16.300023	966.376757	11.470759
16.143862	981.351983	11.475763
15.835660	972.308281	11.480768
16.106737	972.847178	11.485773
16.406175	974.658935	11.490778
16.543200	1002.572572	11.495783
17.026945	1006.558033	11.500787
16.592362	992.368162	11.505792
16.268385	981.415625	11.510797
16.446492	996.241355	11.515802
16.726161	1014.488804	11.520807
17.097628	1005.480188	11.525811
16.686353	1014.963956	11.530816
17.095261	1006.987046	11.535821
16.737688	1008.840515	11.540826
16.819792	1011.822393	11.545831
16.826973	1015.264096	11.550835
16.903604	1017.937753	11.555840
16.628017	1022.148408	11.560845
16.976229	1020.110771	11.565850
16.892090	1014.443978	11.570855
17.054621	1016.003174	11.575859
16.690676	1021.364953	11.580864
16.970532	1033.184462	11.585869
17.284148	1038.095968	11.590874
17.404361	1043.555586	11.595879
17.510692	1043.013692	11.600883
17.191471	1045.744181	11.605888
17.593929	1046.312593	11.610893
17.571099	1053.443017	11.615898
17.389189	1053.357122	11.620903
17.631994	1047.581398	11.625907
17.337002	1054.154385	11.630912
17.226247	1058.091169	11.635917
17.317536	1054.531672	11.640922
17.288036	1074.225750	11.645927
17.766079	1077.021485	11.650931
17.679881	1079.389947	11.655936
17.995044	1085.646427	11.660941
18.099299	1091.936547	11.665946
17.982315	1075.816122	11.670951
17.991088	1074.387728	11.675955
18.058237	1086.512454	11.680960
18.369370	1074.297860	11.685965
18.071537	1081.486352	11.690970
17.997875	1085.753134	11.695975
18.516569	1079.804079	11.700979
18.107962	1090.154835	11.705984
18.068970	1082.444873	11.710989
18.017379	1099.969365	11.715994
18.345651	1101.112611	11.720999
18.468706	1110.870782	11.726003
18.364920	1120.223571	11.731008
18.578702	1115.411284	11.736013
18.754047	1115.993843	11.741018
18.723807	1117.143805	11.746023
19.266445	1114.248781	11.751027
18.782642	1115.633516	11.756032
18.795035	1116.093823	11.761037
18.662233	1111.649067	11.766042
18.799073	1112.811806	11.771047
18.810458	1112.341826	11.776051
18.530881	1122.591597	11.781056
18.944761	1119.379624	11.786061
18.894693	1124.765500	11.791066
18.865797	1127.566400	11.796071
19.072265	1124.005864	11.801075
18.959600	1148.040681	11.806080
19.228630	1149.232805	11.811085
19.271127	1159.383923	11.816090
19.027763	1156.549593	11.821095
19.315630	1151.323335	11.826099
19.077337	1160.468932	11.831104
19.158846	1158.210448	11.836109
19.314688	1163.763781	11.841114
19.267249	1157.791442	11.846119
19.638124	1157.065419	11.851123
19.527173	1177.274124	11.856128
19.527793	1173.451501	11.861133
19.797204	1187.587893	11.866138
19.822996	1184.951916	11.871143
20.027885	1183.785561	11.876147
19.805918	1196.457989	11.881152
20.142290	1187.792344	11.886157
19.933807	1181.263754	11.891162
20.001836	1195.744525	11.896167
20.430479	1180.002189	11.901171
20.297960	1198.478045	11.906176
20.462644	1174.659215	11.911181
20.042569	1170.422693	11.916186
20.155466	1164.850579	11.921191
20.622321	1171.095519	11.926195
20.048131	1175.467389	11.931200
20.302313	1167.207548	11.936205
20.110028	1176.691188	11.941210
20.110608	1185.219930	11.946215
20.561849	1177.023277	11.951219
20.013542	1192.565915	11.956224
20.277058	1186.140248	11.961229
19.815714	1192.817103	11.966234
20.106147	1211.973035	11.971239
20.683892	1221.027946	11.976243
20.605648	1223.631719	11.981248
20.745863	1229.514018	11.986253
20.699933	1212.651938	11.991258
20.533598	1213.541322	11.996263
21.013165	1221.419648	12.001267
20.721741	1228.720738	12.006272
20.925447	1217.059352	12.011277
20.952901	1214.364755	12.016282
20.694602	1225.551121	12.021287
20.611466	1220.819274	12.026291
20.762474	1247.218767	12.031296
21.342763	1247.508076	12.036301
21.178827	1255.820232	12.041306
21.156798	1259.277691	12.046311
21.227652	1230.151205	12.051315
21.157411	1235.376327	12.056320
20.939579	1224.575420	12.061325
20.990680	1224.149568	12.066330
20.737963	1225.648852	12.071335
21.223881	1210.387809	12.076339
20.980273	1232.496004	12.081344
21.280155	1223.818811	12.086349
21.376486	1223.685383	12.091354
21.337876	1215.394937	12.096359
21.446758	1225.740529	12.101363
21.217822	1228.075007	12.106368
21.006175	1218.963708	12.111373
21.036637	1231.375119	12.116378
21.297169	1220.870103	12.121383
21.297006	1228.066388	12.126387
21.198471	1225.773526	12.131392
21.239671	1224.371487	12.136397
20.963729	1214.358914	12.141402
20.952475	1197.803575	12.146407
20.843557	1201.410503	12.151411
20.939214	1210.900283	12.156416
21.377100	1215.569668	12.161421
21.379871	1210.945555	12.166426
21.154568	1205.318549	12.171431
21.446849	1199.556954	12.176435
21.180899	1196.525934	12.181440
21.259281	1195.321405	12.186445
21.053207	1194.971265	12.191450
21.006514	1201.386438	12.196455
21.261214	1183.741543	12.201459
21.145332	1211.418359	12.206464
21.324540	1195.091281	12.211469
20.792049	1205.100734	12.216474
20.934611	1204.969395	12.221479
20.920971	1201.860284	12.226483
21.216164	1199.058329	12.231488
20.957888	1206.522863	12.236493
20.922686	1197.985865	12.241498
21.115055	1199.814728	12.246503
21.101894	1202.124250	12.251507
20.956504	1203.231079	12.256512
20.968638	1194.252848	12.261517
20.983834	1201.527099	12.266522
20.543295	1203.715540	12.271527
20.874032	1197.446313	12.276531
20.845250	1201.302248	12.281536
20.938931	1201.495690	12.286541
20.945641	1206.880427	12.291546
21.260484	1198.885298	12.296551
21.292586	1202.666865	12.301555
20.988814	1216.386895	12.306560
21.063381	1197.611587	12.311565
21.099994	1205.617325	12.316570
20.946617	1206.536183	12.321575
21.207017	1199.918608	12.326579
21.215509	1212.434438	12.331584
21.071626	1202.654715	12.336589
21.001397	1214.006630	12.341594
21.009587	1207.317307	12.346599
21.221473	1206.611908	12.351603
21.006072	1209.333753	12.356608
20.847908	1202.757702	12.361613
20.939536	1217.122761	12.366618
20.975395	1217.669220	12.371623
21.094600	1209.913457	12.376627
21.262260	1211.083905	12.381632
20.983570	1217.525047	12.386637
20.875996	1222.782929	12.391642
20.748955	1219.437997	12.396647
21.175562	1210.470926	12.401651
20.832933	1214.244449	12.406656
20.917880	1214.152263	12.411661
21.260195	1214.921096	12.416666
20.939702	1218.336256	12.421671
20.793917	1211.438086	12.426675
20.721772	1222.006523	12.431680
21.037436	1215.224000	12.436685
20.849416	1218.244272	12.441690
21.225112	1216.364660	12.446695
21.117746	1212.704337	12.451699
21.218836	1227.481083	12.456704
20.980182	1221.192265	12.461709
21.381509	1221.033849	12.466714
21.081935	1221.018760	12.471719
21.196949	1209.783134	12.476723
20.850239	1229.570594	12.481728
21.124398	1213.166847	12.486733
21.008096	1226.732401	12.491738
21.253501	1223.171939	12.496743
21.454616	1221.581960	12.501747
21.018488	1197.422076	12.506752
21.037917	1198.281832	12.511757
21.195313	1184.278070	12.516762
20.883977	1191.025621	12.521767
21.350083	1182.432334	12.526771
20.938386	1197.451691	12.531776
21.132298	1194.484531	12.536781
21.125627	1196.793017	12.541786
20.736402	1196.199261	12.546791
21.299820	1198.699114	12.551795
20.872455	1193.214732	12.556800
21.302757	1197.085762	12.561805
21.631982	1189.421100	12.566810
21.028191	1196.852421	12.571815
21.323556	1187.646085	12.576819
21.268538	1199.299931	12.581824
21.610989	1182.658232	12.586829
21.379798	1182.266364	12.591834
21.129787	1166.146554	12.596839
21.011209	1165.955934	12.601843
20.882297	1159.301116	12.606848
20.834191	1164.171003	12.611853
21.036587	1166.783626	12.616858
21.078339	1162.087076	12.621863
21.028311	1164.952858	12.626867
21.436225	1175.708062	12.631872
21.254000	1149.053894	12.636877
21.249622	1160.177633	12.641882
21.074853	1156.640045	12.646887
21.299404	1155.180382	12.651891
21.270748	1157.616954	12.656896
21.322286	1165.131409	12.661901
21.580947	1150.088032	12.666906
21.115245	1148.615450	12.671911
21.142730	1137.270832	12.676915
21.132451	1142.587287	12.681920
21.146252	1135.999609	12.686925
21.079119	1131.599570	12.691930
20.647895	1136.879076	12.696935
20.959602	1134.863016	12.701939
20.586477	1136.914532	12.706944
20.932711	1153.864682	12.711949
21.186802	1155.576457	12.716954
21.127493	1160.214728	12.721959
20.911763	1146.229510	12.726963
20.704407	1155.196696	12.731968
20.879385	1158.796183	12.736973
21.210849	1152.654599	12.741978
20.788317	1173.031271	12.746983
21.255619	1163.852723	12.751987
21.025737	1170.081045	12.756992
21.093700	1161.311561	12.761997
21.188714	1168.088916	12.767002
20.914416	1166.647309	12.772007
21.150592	1175.840251	12.777011
20.848683	1162.158937	12.782016
20.901652	1172.420363	12.787021
21.105893	1164.863962	12.792026
20.863236	1183.075075	12.797031
21.152408	1169.731590	12.802035
21.244647	1174.568058	12.807040
21.069045	1166.146517	12.812045
21.257513	1156.681267	12.817050
21.201748	1139.973812	12.822055
21.071146	1138.337394	12.827059
20.936121	1143.402496	12.832064
21.086566	1137.472725	12.837069
21.172528	1133.385753	12.842074
20.902557	1138.906060	12.847079
21.091783	1136.895341	12.852083
21.105678	1138.766854	12.857088
20.787945	1136.772332	12.862093
21.172332	1140.158634	12.867098
21.058291	1140.467211	12.872103
21.136728	1139.177518	12.877107
21.213165	1156.896136	12.882112
21.144076	1138.254209	12.887117
21.129915	1149.453622	12.892122
20.843317	1140.840052	12.897127
20.933095	1142.030801	12.902131
21.013071	1132.265887	12.907136
20.854575	1142.169914	12.912141
21.051427	1148.267086	12.917146
20.985441	1144.587565	12.922151
21.165185	1147.110752	12.927155
20.874923	1147.736032	12.932160
21.042008	1144.859897	12.937165
21.436443	1146.541402	12.942170
21.070225	1143.040658	12.947175
21.064133	1150.616339	12.952179
21.075724	1148.605562	12.957184
20.811684	1153.743287	12.962189
21.230622	1151.479874	12.967194
20.869517	1151.293241	12.972199
21.273787	1145.445993	12.977203
21.147677	1151.752379	12.982208
20.835340	1148.955860	12.987213
21.054831	1146.558670	12.992218
21.052108	1152.717638	12.997223
21.128420	1137.443147	13.002227
21.308213	1153.410541	13.007232
20.909201	1145.524563	13.012237
21.285642	1151.118406	13.017242
20.680276	1157.252060	13.022247
20.921332	1145.531155	13.027251
21.116662	1152.705686	13.032256
20.859996	1146.670522	13.037261
21.232026	1151.572751	13.042266
21.011467	1154.736979	13.047271
20.989311	1146.095423	13.052275
21.148358	1148.025793	13.057280
21.154558	1149.266144	13.062285
21.118714	1153.992140	13.067290
20.882263	1156.654251	13.072295
20.956948	1149.990621	13.077299
20.980831	1158.849962	13.082304
20.884110	1151.351030	13.087309
21.107284	1153.206515	13.092314
20.605409	1159.842508	13.097319
20.577664	1157.213498	13.102323
20.643775	1158.622500	13.107328
21.041125	1166.946017	13.112333
21.154680	1153.004473	13.117338
20.839118	1166.155450	13.122343
20.892430	1161.149534	13.127347
20.982396	1162.056388	13.132352
20.952798	1169.607441	13.137357
21.225356	1153.170899	13.142362
20.921265	1161.229374	13.147367
21.163620	1154.915911	13.152371
21.224464	1167.992663	13.157376
21.227998	1163.442564	13.162381
21.275708	1155.863821	13.167386
20.855788	1161.221962	13.172391
21.385438	1159.581168	13.177395
21.349604	1160.604285	13.182400
21.091334	1160.686693	13.187405
21.260902	1156.505952	13.192410
20.903916	1153.767019	13.197415
21.026581	1157.974122	13.202419
21.110158	1164.874731	13.207424
21.144915	1151.112923	13.212429
21.334315	1140.236090	13.217434
20.944103	1134.993399	13.222439
20.920945	1125.412104	13.227443
20.820723	1134.278608	13.232448
20.945205	1129.589375	13.237453
21.290145	1143.584361	13.242458
20.978871	1140.406032	13.247463
21.214969	1133.740321	13.252467
21.066519	1137.025515	13.257472
20.935043	1128.111232	13.262477
21.081377	1133.325432	13.267482
20.716764	1132.311416	13.272487
21.096764	1127.595624	13.277491
20.878241	1128.903355	13.282496
20.797326	1129.408508	13.287501
21.610238	1137.325091	13.292506
20.698456	1144.404942	13.297511
21.154370	1134.045454	13.302515
21.104908	1134.824725	13.307520
21.239197	1132.480552	13.312525
21.212693	1124.284427	13.317530
21.081682	1130.642050	13.322535
21.518623	1129.367723	13.327539
21.036556	1131.799332	13.332544
20.907307	1125.655541	13.337549
21.351860	1126.367061	13.342554
21.143382	1133.345775	13.347559
21.219955	1125.049626	13.352563
21.040038	1132.998391	13.357568
20.948627	1133.431098	13.362573
21.071668	1133.381724	13.367578
20.885982	1136.553002	13.372583
20.784054	1143.088929	13.377587
21.000651	1136.475215	13.382592
21.142827	1133.241914	13.387597
21.122308	1139.326440	13.392602
21.215581	1129.076835	13.397607
20.906759	1138.161123	13.402611
20.623337	1141.942532	13.407616
20.856618	1128.481837	13.412621
21.226123	1137.210344	13.417626
20.794113	1137.538093	13.422631
21.365313	1141.763546	13.427635
21.328645	1136.677367	13.432640
20.883915	1143.987095	13.437645
21.202596	1143.693619	13.442650
21.117972	1139.987107	13.447655
21.224432	1135.565688	13.452659
21.217625	1142.996392	13.457664
21.253685	1133.405647	13.462669
21.108873	1122.575822	13.467674
21.013760	1121.244421	13.472679
20.994377	1110.859825	13.477683
20.637926	1104.853210	13.482688
20.807334	1114.433672	13.487693
21.100892	1121.480551	13.492698
21.332265	1142.866273	13.497703
21.207964	1124.310444	13.502707
21.040909	1118.915468	13.507712
20.920804	1112.435894	13.512717
21.012430	1109.598610	13.517722
20.726836	1110.525933	13.522727
20.936034	1128.639680	13.527731
21.258911	1139.195520	13.532736
20.853531	1133.584646	13.537741
20.795573	1120.198795	13.542746
21.017030	1138.173396	13.547751
21.169723	1137.441169	13.552755
21.207456	1148.665422	13.557760
20.879183	1138.061975	13.562765
21.134622	1124.212954	13.567770
20.499240	1132.813131	13.572775
20.871488	1131.240024	13.577779
20.974995	1133.750135	13.582784
20.830970	1140.163458	13.587789
21.084189	1138.279734	13.592794
21.256716	1141.906418	13.597799
21.500598	1139.423333	13.602803
21.192970	1141.779810	13.607808
20.892936	1138.777894	13.612813
21.316956	1117.753302	13.617818
20.835176	1114.835573	13.622823
21.222475	1118.724479	13.627827
21.248553	1118.113377	13.632832
20.954492	1109.748610	13.637837
21.139366	1114.328998	13.642842
20.771642	1116.800717	13.647847
20.919018	1108.146339	13.652851
20.817136	1115.841363	13.657856
20.521694	1113.255056	13.662861
20.946610	1114.222032	13.667866
20.901055	1152.095641	13.672871
20.993889	1133.908890	13.677875
21.279951	1152.314774	13.682880
21.098968	1148.358687	13.687885
21.298317	1138.383909	13.692890
21.232488	1140.610354	13.697895
21.147168	1113.379372	13.702899
20.898329	1127.439081	13.707904
20.706564	1114.013071	13.712909
21.121290	1116.900919	13.717914
20.887592	1121.538605	13.722919
20.829748	1119.042142	13.727923
20.855595	1137.215106	13.732928
21.082182	1143.730178	13.737933
21.083135	1139.402860	13.742938
20.956703	1151.112214	13.747943
20.823831	1148.000052	13.752947
21.196336	1152.183078	13.757952
21.025783	1148.401955	13.762957
21.074366	1149.332756	13.767962
21.175519	1150.494882	13.772967
21.023192	1146.135235	13.777971
20.853203	1146.416463	13.782976
20.591302	1148.314617	13.787981
21.194742	1146.704635	13.792986
20.668751	1155.470315	13.797991
20.817597	1153.191629	13.802995
21.091864	1153.827802	13.808000
20.803346	1159.185487	13.813005
21.330820	1143.635595	13.818010
21.201238	1156.430455	13.823015
21.184774	1142.853452	13.828019
21.034446	1150.212427	13.833024
20.939990	1151.571339	13.838029
21.272765	1159.419424	13.843034
21.055690	1162.220380	13.848039
21.109261	1154.364722	13.853043
21.167389	1149.435317	13.858048
20.855634	1144.528635	13.863053
20.964764	1142.207397	13.868058
21.088728	1155.507472	13.873063
21.303357	1150.646151	13.878067
21.035260	1138.580658	13.883072
20.891033	1126.864445	13.888077
21.259737	1128.203104	13.893082
21.150682	1130.789697	13.898087
20.917041	1127.966438	13.903091
20.921722	1125.365380	13.908096
21.027933	1131.152132	13.913101
21.060900	1122.561726	13.918106
20.959903	1127.686054	13.923111
20.915842	1135.029650	13.928115
20.764149	1137.085276	13.933120
20.919003	1124.474497	13.938125
20.824299	1148.329823	13.943130
20.956923	1157.111892	13.948135
21.236404	1165.824811	13.953139
21.337630	1160.730824	13.958144
21.176766	1147.186310	13.963149
21.373606	1138.553988	13.968154
21.304191	1132.695556	13.973159
21.412156	1139.513412	13.978163
21.079050	1127.628616	13.983168
20.968514	1148.434910	13.988173
21.369376	1126.858882	13.993178
21.238061	1136.135642	13.998183
21.201089	1142.569741	14.003187
21.329150	1137.372130	14.008192
21.102600	1146.103509	14.013210
21.323477	1130.969172	14.018227
21.090860	1118.933645	14.023245
21.111085	1105.037833	14.028263
21.153608	1113.744151	14.033280
21.014111	1097.912281	14.038298
21.013435	1104.651361	14.043315
20.642797	1112.962683	14.048333
21.012305	1120.245192	14.053351
21.355917	1128.765074	14.058368
21.008491	1139.905699	14.063386
21.000306	1135.957390	14.068403
21.410203	1139.659589	14.073421
21.329368	1137.914071	14.078439
21.278786	1150.396328	14.083456
21.181655	1148.826439	14.088474
21.388059	1137.232105	14.093491
21.216059	1146.129959	14.098509
21.161032	1134.701591	14.103527
21.198004	1134.656584	14.108544
21.306720	1147.267587	14.113562
21.206580	1139.222093	14.118579
20.895032	1138.907058	14.123597
21.341166	1142.867744	14.128615
21.241098	1143.294474	14.133632
21.141311	1138.393373	14.138650
21.467041	1137.231092	14.143667
21.337888	1142.501040	14.148685
21.219922	1162.690798	14.153703
21.159676	1165.299238	14.158720
21.182134	1178.664915	14.163738
21.166638	1168.633345	14.168755
21.267273	1172.647570	14.173773
21.305415	1168.378834	14.178791
21.491676	1179.950320	14.183808
21.117050	1183.271144	14.188826
21.660034	1201.073095	14.193843
21.415691	1210.481171	14.198861
21.374827	1211.916203	14.203879
21.607645	1208.110335	14.208896
21.670539	1204.339434	14.213914
21.655484	1215.703957	14.218931
21.835234	1208.946132	14.223949
21.713027	1212.270748	14.228967
21.742840	1207.138169	14.233984
21.664659	1202.596968	14.239002
21.826824	1199.194051	14.244019
21.527481	1212.255581	14.249037
21.431176	1218.014246	14.254055
21.702473	1220.874984	14.259072
21.784003	1236.675764	14.264090
21.636449	1237.953209	14.269107
21.775587	1241.244015	14.274125
22.015573	1236.384645	14.279143
21.989590	1238.564491	14.284160
21.983658	1243.460894	14.289178
22.299633	1248.502585	14.294195
22.033945	1242.441850	14.299213
22.228902	1251.871124	14.304231
22.124306	1235.866796	14.309248
21.699475	1249.058485	14.314266
22.348440	1237.451690	14.319283
22.331312	1238.472380	14.324301
22.379390	1239.989184	14.329319
22.597850	1240.777247	14.334336
22.280527	1228.368175	14.339354
22.280782	1215.309144	14.344371
22.094746	1216.051607	14.349389
21.645143	1205.483635	14.354407
22.408167	1222.097496	14.359424
22.298097	1235.226387	14.364442
22.230756	1237.551255	14.369459
22.694329	1250.643724	14.374477
21.877493	1241.183503	14.379495
22.698696	1238.296811	14.384512
22.280665	1248.536427	14.389530
22.227863	1237.412790	14.394547
22.511148	1238.048941	14.399565
22.120827	1241.853625	14.404583
22.466404	1240.044805	14.409600
22.262915	1246.391582	14.414618
22.424891	1240.824208	14.419635
22.371370	1245.500114	14.424653
22.365898	1236.215657	14.429671
22.364894	1243.451928	14.434688
22.305664	1245.745617	14.439706
22.661173	1239.922435	14.444723
22.696320	1241.417706	14.449741
22.244773	1247.277084	14.454759
22.682239	1238.632987	14.459776
22.893265	1242.105809	14.464794
22.914832	1240.886639	14.469811
22.648067	1246.263515	14.474829
22.569160	1239.142662	14.479847
23.002966	1248.305753	14.484864
22.749282	1252.250668	14.489882
22.846611	1247.791572	14.494899
22.517506	1245.877998	14.499917
22.198205	1259.757579	14.504935
22.339079	1264.097319	14.509952
22.529612	1287.585442	14.514970
22.624381	1280.875744	14.519987
22.605345	1279.884842	14.525005
22.533088	1285.979471	14.530023
23.107378	1279.649473	14.535040
22.625780	1279.551891	14.540058
22.850183	1272.561972	14.545075
23.078503	1297.640705	14.550093
23.130427	1297.008146	14.555111
23.369768	1290.676507	14.560128
23.213935	1288.559113	14.565146
23.233986	1277.378209	14.570163
22.925437	1277.416623	14.575181
22.965617	1284.770616	14.580199
23.176686	1280.823479	14.585216
23.171027	1279.176065	14.590234
22.986126	1278.197460	14.595251
23.122261	1287.266478	14.600269
23.066665	1299.990336	14.605287
23.679344	1298.014640	14.610304
23.271083	1288.544279	14.615322
23.247901	1281.574966	14.620339
23.376053	1284.353155	14.625357
23.149121	1293.119859	14.630375
23.155864	1281.263100	14.635392
23.176140	1294.257996	14.640410
23.466292	1313.912538	14.645427
23.777766	1306.164673	14.650445
23.351777	1302.713964	14.655463
23.447269	1290.007765	14.660480
23.093260	1296.405312	14.665498
23.080098	1312.255883	14.670515
23.592775	1312.245117	14.675533
23.442340	1311.754944	14.680551
23.670031	1308.366720	14.685568
23.588264	1310.483115	14.690586
23.697716	1312.174182	14.695603
23.604483	1299.790658	14.700621
23.609797	1315.842780	14.705639
23.573648	1302.778465	14.710656
23.486514	1314.252089	14.715674
23.646295	1309.561217	14.720691
23.790269	1314.109691	14.725709
23.609062	1316.111385	14.730727
23.795172	1307.077900	14.735744
23.620580	1319.897832	14.740762
23.647322	1314.515594	14.745779
24.082355	1316.920800	14.750797
23.743345	1321.429903	14.755815
23.800990	1318.257561	14.760832
23.930314	1307.002577	14.765850
24.068649	1312.739586	14.770867
24.086465	1317.204362	14.775885
23.635732	1321.822520	14.780903
24.222643	1307.408271	14.785920
23.756716	1308.078973	14.790938
23.562332	1310.433553	14.795955
23.930623	1312.217046	14.800973
23.694445	1310.474260	14.805991
24.017379	1304.977145	14.811008
23.783327	1312.271069	14.816026
23.861059	1324.022001	14.821043
24.128172	1319.745017	14.826061
23.670347	1340.012820	14.831079
24.200511	1334.348935	14.836096
24.154729	1348.139359	14.841114
24.066764	1344.935178	14.846131
24.412573	1339.105638	14.851149
24.244760	1350.233507	14.856167
24.298548	1349.229413	14.861184
24.360221	1339.954630	14.866202
24.470957	1351.959872	14.871219
24.549199	1340.873458	14.876237
24.401867	1343.034921	14.881255
24.455291	1309.484887	14.886272
24.301954	1318.293351	14.891290
24.283681	1314.919186	14.896307
24.490873	1313.171754	14.901325
24.099365	1319.992144	14.906343
24.406811	1333.060825	14.911360
24.688857	1336.805489	14.916378
24.534972	1347.670011	14.921395
24.762666	1340.602456	14.926413
24.720870	1342.223268	14.931431
24.659174	1318.831341	14.936448
24.545729	1307.649682	14.941466
24.315239	1319.352241	14.946483
24.944348	1318.235942	14.951501
24.481636	1327.515326	14.956519
24.653185	1328.287280	14.961536
24.496188	1338.963528	14.966554
24.482368	1343.552908	14.971571
24.579526	1344.258076	14.976589
24.453704	1349.378130	14.981607
24.867467	1342.335954	14.986624
24.726875	1353.898360	14.991642
24.545014	1345.857920	14.996659
24.845524	1346.145263	15.001677
24.727012	1347.545501	15.006695
24.723553	1348.694581	15.011712
25.060945	1343.361888	15.016730
24.967500	1333.750052	15.021747
25.024690	1339.849226	15.026765
24.835783	1344.936868	15.031783
25.173153	1338.410249	15.036800
25.147416	1338.990298	15.041818
24.770693	1350.376429	15.046835
24.858370	1334.800652	15.051853
24.838994	1340.452714	15.056871
24.944266	1341.123553	15.061888
24.760319	1350.953098	15.066906
24.969703	1356.917895	15.071923
25.111975	1379.984426	15.076941
25.130571	1378.363020	15.081959
24.870997	1382.643967	15.086976
25.531030	1370.226762	15.091994
25.305988	1382.254120	15.097011
25.516352	1369.572003	15.102029
25.326382	1381.172194	15.107047
25.429779	1371.200174	15.112064
25.447713	1384.066535	15.117082
25.290745	1382.438523	15.122099
25.446772	1376.082382	15.127117
25.442712	1373.239196	15.132135
25.477656	1366.463494	15.137152
25.438280	1371.771117	15.142170
25.356839	1375.844325	15.147187
25.668864	1374.622863	15.152205
25.635857	1377.637560	15.157223
25.504711	1378.564759	15.162240
25.678080	1374.128104	15.167258
25.317300	1390.775101	15.172275
25.821438	1370.618249	15.177293
25.530741	1388.954519	15.182311
25.644955	1366.270642	15.187328
25.786746	1377.808479	15.192346
25.686950	1375.365955	15.197363
25.815022	1381.946203	15.202381
25.669810	1384.571380	15.207399
25.698333	1392.427512	15.212416
25.841778	1379.392687	15.217434
25.337662	1379.075325	15.222451
25.912274	1378.403445	15.227469
25.694823	1385.056104	15.232487
25.818059	1375.672379	15.237504
25.948270	1375.334073	15.242522
25.649247	1376.865351	15.247539
25.641112	1381.420803	15.252557
25.998320	1379.166515	15.257575
25.858569	1377.194408	15.262592
25.754688	1388.296379	15.267610
25.493906	1394.406964	15.272627
26.024461	1377.129268	15.277645
26.149503	1401.785775	15.282663
25.964521	1397.245816	15.287680
26.241583	1407.321200	15.292698
26.143351	1422.123657	15.297715
26.142999	1418.565710	15.302733
26.451266	1421.815426	15.307751
26.167365	1394.302844	15.312768
26.324513	1394.831704	15.317786
25.974494	1403.753387	15.322803
26.427490	1408.373729	15.327821
26.354169	1418.531745	15.332839
26.135749	1420.522084	15.337856
26.679558	1411.362272	15.342874
26.248232	1409.855092	15.347891
26.483737	1400.763334	15.352909
26.590322	1409.253544	15.357927
26.398883	1410.818004	15.362944
26.244707	1401.280304	15.367962
26.502352	1413.808010	15.372979
26.643363	1413.043260	15.377997
26.520462	1416.187133	15.383015
26.459811	1421.856821	15.388032
26.784799	1414.484273	15.393050
26.386522	1413.163733	15.398067
26.604159	1407.853263	15.403085
26.584771	1422.105166	15.408103
26.390084	1420.008107	15.413120
26.735281	1413.889196	15.418138
26.660660	1419.885157	15.423155
26.643033	1405.724532	15.428173
26.683643	1407.525692	15.433191
26.190131	1413.203064	15.438208
26.590073	1411.173192	15.443226
26.719530	1405.848471	15.448243
26.756274	1413.506674	15.453261
26.606036	1416.390636	15.458279
26.641407	1415.096890	15.463296
26.641792	1417.777503	15.468314
26.565484	1438.588642	15.473331
27.069947	1431.429711	15.478349
26.829011	1435.662082	15.483367
26.847838	1431.239045	15.488384
26.613619	1443.683201	15.493402
26.836311	1436.842916	15.498419
26.802504	1436.165822	15.503437
26.789987	1442.457057	15.508455
26.962890	1430.148954	15.513472
27.512815	1435.018117	15.518490
27.139484	1443.706012	15.523507
27.183383	1433.169279	15.528525
27.272573	1434.917075	15.533543
27.176679	1430.240200	15.538560
27.393018	1434.253348	15.543578
27.399946	1440.505301	15.548595
27.390886	1435.429179	15.553613
27.436296	1437.314521	15.558631
27.439681	1439.126341	15.563648
27.562405	1426.841974	15.568666
27.010707	1436.090000	15.573683
27.294334	1449.706858	15.578701
27.578105	1450.847890	15.583719
27.511992	1463.567276	15.588736
27.912989	1458.718333	15.593754
28.126411	1454.895045	15.598771
28.136445	1422.114598	15.603789
27.925961	1421.884111	15.608807
27.651892	1417.473186	15.613824
28.013672	1421.782461	15.618842
27.556487	1432.479912	15.623859
27.873051	1426.842195	15.628877
27.619350	1425.895002	15.633895
27.791536	1430.610475	15.638912
27.715028	1424.753874	15.643930
27.580731	1432.904986	15.648947
27.749948	1424.956375	15.653965
27.603727	1421.752030	15.658983
27.883656	1422.585356	15.664000
27.690615	1411.863054	15.669018
27.338955	1420.814897	15.674035
27.786994	1420.694890	15.679053
27.706745	1424.184324	15.684071
27.775712	1445.541744	15.689088
28.162673	1446.022943	15.694106
28.280237	1448.914538	15.699123
28.254456	1448.333692	15.704141
27.916209	1422.248610	15.709159
27.830850	1434.706769	15.714176
27.983960	1457.293490	15.719194
27.984659	1466.852988	15.724211
27.946886	1466.053828	15.729229
28.147451	1451.063972	15.734247
28.132996	1465.195580	15.739264
28.344606	1461.666738	15.744282
28.323727	1462.239725	15.749299
28.410207	1461.965022	15.754317
28.168075	1455.747854	15.759335
28.393309	1458.545200	15.764352
28.337827	1453.929512	15.769370
27.915593	1463.156907	15.774387
28.302843	1457.072171	15.779405
28.408656	1459.378897	15.784423
28.263534	1463.089474	15.789440
28.288844	1461.103615	15.794458
28.210645	1472.520882	15.799475
28.250475	1481.633696	15.804493
28.715955	1486.966237	15.809511
28.667980	1502.849310	15.814528
28.929597	1479.945116	15.819546
28.668232	1494.284447	15.824563
28.853140	1491.985262	15.829581
28.852570	1474.046535	15.834599
28.688244	1468.850444	15.839616
28.669372	1452.898273	15.844634
28.942685	1464.984645	15.849651
28.979385	1466.581940	15.854669
29.208890	1454.329284	15.859687
28.715199	1455.359928	15.864704
29.244965	1449.104600	15.869722
29.062367	1448.300223	15.874739
28.839638	1458.040070	15.879757
29.015735	1447.024486	15.884775
28.848896	1456.668900	15.889792
28.769871	1455.851151	15.894810
28.636259	1456.833805	15.899827
28.957619	1464.772262	15.904845
29.348959	1469.657291	15.909863
29.227436	1478.065944	15.914880
29.439201	1477.982047	15.919898
29.297074	1466.118992	15.924915
28.873249	1460.589906	15.929933
29.398864	1456.946491	15.934951
29.365423	1467.971220	15.939968
29.315371	1448.999059	15.944986
29.089351	1444.110122	15.950003
29.270426	1466.008123	15.955021
29.391852	1469.177536	15.960039
29.288999	1479.944353	15.965056
29.311559	1479.673552	15.970074
29.327965	1483.823995	15.975091
29.313969	1492.357080	15.980109
29.995533	1484.125374	15.985127
29.700455	1474.762683	15.990144
29.270446	1465.116346	15.995162
29.840479	1475.083704	16.000179
29.306311	1474.918997	16.005197
29.602349	1470.966123	16.010215
29.735608	1480.724715	16.015232
29.471784	1480.400486	16.020250
29.807260	1476.760650	16.025267
29.642308	1482.319578	16.030285
29.739808	1472.705511	16.035303
29.708372	1480.692378	16.040320
29.599341	1468.946740	16.045338
29.691825	1485.320206	16.050355
29.459596	1483.708904	16.055373
29.441960	1484.271936	16.060391
29.571691	1480.987387	16.065408
29.411532	1485.414532	16.070426
29.344787	1489.282504	16.075443
29.872489	1503.319816	16.080461
29.962125	1516.654640	16.085479
29.918139	1526.493442	16.090496
30.095865	1511.787170	16.095514
30.388844	1510.018168	16.100531
30.109867	1517.939141	16.105549
30.604024	1501.897229	16.110567
30.178906	1520.385665	16.115584
30.188795	1512.344439	16.120602
30.396409	1505.066072	16.125619
30.067502	1511.406224	16.130637
30.370746	1500.214590	16.135655
30.134580	1505.792751	16.140672
30.186526	1516.163667	16.145690
30.315117	1507.252492	16.150707
30.478878	1510.026618	16.155725
30.680880	1498.994279	16.160743
30.404825	1517.197811	16.165760
30.536810	1512.951761	16.170778
30.791523	1507.868152	16.175795
30.236984	1518.949287	16.180813
30.842793	1510.268744	16.185831
30.799062	1513.591924	16.190848
30.510508	1515.181322	16.195866
30.553267	1511.276697	16.200883
30.426062	1514.806675	16.205901
30.490283	1516.387002	16.210919
30.509207	1515.496998	16.215936
30.270805	1512.201939	16.220954
30.442543	1496.760450	16.225971
30.336461	1514.870802	16.230989
30.507716	1500.162428	16.236007
30.563878	1513.952480	16.241024
30.776996	1520.402822	16.246042
31.038783	1536.475632	16.251059
30.959003	1539.252426	16.256077
31.217615	1539.294767	16.261095
31.117076	1525.713548	16.266112
31.094700	1510.166147	16.271130
31.258261	1502.212104	16.276147
30.781996	1517.284165	16.281165
30.929303	1509.438105	16.286183
30.825365	1518.169597	16.291200
30.825198	1535.171386	16.296218
31.232670	1532.786361	16.301235
30.963634	1541.578805	16.306253
31.163726	1530.988775	16.311271
31.097682	1542.375843	16.316288
31.040088	1538.507666	16.321306
31.185287	1536.307617	16.326323
31.163927	1538.835989	16.331341
31.317129	1541.673154	16.336359
31.591246	1535.387775	16.341376
31.374886	1536.696669	16.346394
31.388409	1528.052375	16.351411
31.399277	1523.430802	16.356429
31.460486	1528.349627	16.361447
31.356432	1527.449347	16.366464
31.313939	1531.348070	16.371482
31.550956	1534.689401	16.376499
31.450149	1569.325485	16.381517
31.690453	1566.460591	16.386535
31.899968	1563.661958	16.391552
31.868378	1570.656301	16.396570
32.043199	1552.999396	16.401587
31.564368	1541.306385	16.406605
31.821160	1537.977962	16.411623
32.056832	1547.037561	16.416640
31.746639	1540.953909	16.421658
31.799210	1522.182367	16.426675
31.685928	1549.974475	16.431693
31.985834	1547.523231	16.436711
32.122967	1558.772514	16.441728
32.247218	1560.118325	16.446746
31.948825	1543.510624	16.451763
32.181347	1554.890984	16.456781
32.018429	1537.747295	16.461799
32.118052	1544.533505	16.466816
32.178787	1545.268088	16.471834
32.551655	1530.343481	16.476851
31.994148	1532.425668	16.481869
31.777673	1526.552022	16.486887
32.225499	1545.165539	16.491904
32.353576	1554.198257	16.496922
32.298396	1545.445357	16.501939
32.397923	1551.152471	16.506957
32.584696	1549.711868	16.511975
32.422633	1537.403613	16.516992
32.472810	1548.004500	16.522010
32.813347	1546.515778	16.527027
32.188864	1534.836563	16.532045
32.369896	1533.513283	16.537063
32.534553	1543.515452	16.542080
32.282829	1553.046051	16.547098
32.904384	1541.363164	16.552115
32.532397	1552.894990	16.557133
32.657238	1549.669409	16.562151
32.748525	1556.828195	16.567168
32.548472	1553.040937	16.572186
33.058437	1542.483277	16.577203
32.916400	1546.415184	16.582221
32.629186	1545.968839	16.587239
32.976790	1547.258577	16.592256
32.895236	1533.106450	16.597274
33.067999	1545.539268	16.602291
32.936887	1553.759154	16.607309
32.950649	1548.430810	16.612327
33.039545	1543.274533	16.617344
32.862566	1552.338598	16.622362
32.917805	1534.430221	16.627379
32.834350	1548.903256	16.632397
32.918927	1549.064591	16.637415
33.163373	1547.284448	16.642432
32.983394	1553.537944	16.647450
33.037223	1548.797825	16.652467
32.723980	1546.106164	16.657485
33.006642	1544.041496	16.662503
33.526008	1542.533692	16.667520
33.207070	1543.566358	16.672538
33.190305	1542.807888	16.677555
33.198888	1533.067961	16.682573
32.917987	1542.669274	16.687591
33.115145	1550.014096	16.692608
33.157183	1575.399877	16.697626
33.031317	1564.638434	16.702643
33.229171	1579.510236	16.707661
32.965266	1576.845307	16.712679
33.261157	1576.803050	16.717696
33.131796	1604.437374	16.722714
33.640266	1604.729311	16.727731
33.924466	1601.563247	16.732749
34.083630	1601.501897	16.737767
34.281512	1600.397725	16.742784
34.043189	1587.165620	16.747802
34.194483	1568.379846	16.752819
34.092576	1564.222994	16.757837
33.914376	1566.553011	16.762855
34.152356	1557.408850	16.767872
33.909461	1569.494266	16.772890
33.754856	1560.593617	16.777907
33.764632	1558.852472	16.782925
33.908057	1567.926796	16.787943
33.995827	1560.799652	16.792960
33.886349	1574.244938	16.797978
34.099900	1556.754888	16.802995
33.838448	1568.759891	16.808013
33.813916	1566.284881	16.813031
34.003716	1560.261482	16.818048
33.869098	1584.826003	16.823066
34.080299	1591.737588	16.828083
34.120958	1600.823603	16.833101
34.080483	1600.437008	16.838119
34.335679	1598.309072	16.843136
34.134814	1595.750492	16.848154
34.390671	1609.784072	16.853171
34.318062	1594.337403	16.858189
34.043569	1599.128889	16.863207
34.604834	1589.313364	16.868224
34.514149	1603.705807	16.873242
34.572677	1591.846827	16.878259
34.606787	1599.821733	16.883277
34.568298	1598.879531	16.888295
34.527063	1591.063497	16.893312
34.318188	1593.283576	16.898330
34.900895	1598.792523	16.903347
34.730980	1613.087497	16.908365
35.112693	1621.551257	16.913383
34.975093	1595.465323	16.918400
34.483005	1600.165668	16.923418
34.547975	1609.194327	16.928435
34.714187	1608.263523	16.933453
34.872429	1620.634226	16.938471
34.857357	1617.311390	16.943488
34.778727	1619.568905	16.948506
35.095051	1627.803991	16.953523
35.098406	1623.532805	16.958541
35.131010	1630.112661	16.963559
35.400950	1619.133892	16.968576
35.289989	1618.885956	16.973594
35.501480	1625.361773	16.978611
35.575069	1611.524609	16.983629
35.245850	1620.771875	16.988647
35.571955	1612.963313	16.993664
35.429937	1616.862201	16.998682
35.552343	1600.166874	17.003699
35.386933	1590.471960	17.008717
35.284896	1590.187994	17.013735
35.756155	1586.800188	17.018752
35.406900	1583.494477	17.023770
35.257272	1603.828325	17.028787
35.317450	1595.601276	17.033805
35.686294	1608.853902	17.038823
35.761233	1612.587624	17.043840
35.618765	1615.943877	17.048858
35.822648	1619.235456	17.053875
35.856693	1604.015591	17.058893
35.584056	1604.765591	17.063911
35.702335	1590.646033	17.068928
35.600484	1607.244117	17.073946
35.232535	1610.195873	17.078963
35.903552	1610.633350	17.083981
35.795171	1622.414206	17.088999
36.181991	1617.015328	17.094016
35.762008	1625.246718	17.099034
36.173756	1611.500344	17.104051
36.065187	1612.530925	17.109069
35.633598	1633.444623	17.114087
36.193852	1611.683403	17.119104
36.111709	1618.036157	17.124122
35.716512	1616.910164	17.129139
35.841400	1611.166090	17.134157
35.756805	1623.685639	17.139175
35.928957	1611.305142	17.144192
35.887363	1645.714882	17.149210
36.240635	1645.786173	17.154227
36.556926	1640.590449	17.159245
36.376789	1642.173580	17.164263
36.431912	1639.152585	17.169280
36.503638	1647.755463	17.174298
36.448176	1640.652697	17.179315
36.535713	1646.141531	17.184333
36.357483	1639.929823	17.189351
36.381504	1634.996223	17.194368
36.319363	1649.047523	17.199386
36.556105	1638.107069	17.204403
36.506740	1641.382411	17.209421
36.043521	1635.433239	17.214439
36.731102	1654.914746	17.219456
36.731360	1668.822402	17.224474
36.929345	1671.245027	17.229491
36.961433	1676.154388	17.234509
36.866226	1665.521691	17.239527
37.380709	1656.723491	17.244544
36.976425	1652.196403	17.249562
36.911638	1645.736932	17.254579
37.119110	1623.978473	17.259597
36.648049	1640.942225	17.264615
36.929078	1642.590238	17.269632
36.949444	1659.131135	17.274650
36.841424	1666.685140	17.279667
37.131780	1665.234299	17.284685
37.124792	1670.503830	17.289703
37.514466	1662.011831	17.294720
37.622210	1669.986043	17.299738
37.150309	1666.152446	17.304755
37.480938	1662.530641	17.309773
37.449933	1666.185316	17.314791
37.525267	1672.999056	17.319808
37.504470	1666.090528	17.324826
37.471538	1664.082469	17.329843
37.513627	1668.551347	17.334861
37.334941	1676.514614	17.339879
37.465593	1662.039074	17.344896
37.416957	1661.757601	17.349914
37.223359	1669.021654	17.354931
37.833575	1653.711420	17.359949
37.379052	1671.360000	17.364967
37.269942	1656.044932	17.369984
37.616765	1664.666869	17.375002
37.691716	1687.999464	17.380019
38.051133	1697.155829	17.385037
38.246163	1694.250940	17.390055
38.215745	1679.851408	17.395072
38.071825	1671.917996	17.400090
37.877070	1668.674143	17.405107
38.034442	1652.945335	17.410125
38.074578	1661.600452	17.415143
37.731376	1660.146830	17.420160
38.124579	1685.542867	17.425178
37.856379	1686.918245	17.430195
37.994088	1691.175247	17.435213
37.717674	1702.544080	17.440231
37.983080	1695.991026	17.445248
37.725339	1697.457548	17.450266
37.850642	1708.251070	17.455283
38.371038	1707.663334	17.460301
38.182388	1725.818579	17.465319
38.248616	1725.588787	17.470336
38.593496	1729.802535	17.475354
38.483418	1724.535564	17.480371
38.846179	1721.272787	17.485389
38.755616	1719.538187	17.490407
38.725237	1724.695848	17.495424
38.366717	1720.704150	17.500442
38.484341	1727.195770	17.505459
39.061625	1723.784732	17.510477
39.022867	1724.473841	17.515495
38.869539	1720.984263	17.520512
38.947365	1724.025401	17.525530
38.716175	1714.683825	17.530547
39.005220	1718.904115	17.535565
38.768678	1721.350429	17.540583
38.923267	1712.291832	17.545600
39.195023	1714.511571	17.550618
39.022206	1722.160098	17.555635
39.158238	1711.794878	17.560653
38.997704	1710.643251	17.565671
38.911330	1714.821949	17.570688
39.168076	1706.680682	17.575706
39.086727	1717.957068	17.580723
39.213271	1704.803521	17.585741
39.060096	1713.343203	17.590759
39.123769	1714.533517	17.595776
39.250305	1719.782558	17.600794
39.184868	1738.825045	17.605811
39.283326	1741.254903	17.610829
39.336564	1748.448954	17.615847
38.960768	1742.433097	17.620864
39.379318	1733.107440	17.625882
39.656636	1735.482029	17.630899
39.874551	1739.590969	17.635917
39.950559	1740.482007	17.640935
39.882610	1743.714717	17.645952
40.165422	1737.767649	17.650970
40.017554	1743.166644	17.655987
39.967622	1733.814239	17.661005
40.001926	1732.916263	17.666023
39.779504	1734.807391	17.671040
39.932503	1726.932778	17.676058
40.152516	1738.897316	17.681075
39.993739	1725.273286	17.686093
39.991206	1727.469916	17.691111
39.971054	1730.617132	17.696128
40.198782	1729.666286	17.701146
40.135766	1749.944051	17.706163
39.990504	1740.362232	17.711181
40.137611	1736.512480	17.716199
40.032900	1741.501098	17.721216
40.376753	1733.791104	17.726234
40.178327	1736.104709	17.731251
40.410898	1736.398178	17.736269
40.065617	1736.861672	17.741287
40.501773	1743.775208	17.746304
40.356322	1732.025726	17.751322
40.075135	1743.265574	17.756339
40.306205	1736.025038	17.761357
40.354990	1747.513508	17.766375
40.190778	1747.026302	17.771392
40.346067	1755.299729	17.776410
40.378260	1771.086150	17.781427
40.535021	1768.548371	17.786445
40.464716	1770.445919	17.791463
40.614557	1773.488953	17.796480
40.671552	1763.957448	17.801498
40.836448	1762.578518	17.806515
40.888420	1754.528086	17.811533
40.955520	1772.595409	17.816551
40.840865	1769.355277	17.821568
41.312540	1767.818878	17.826586
41.419095	1773.920587	17.831603
41.367528	1767.043661	17.836621
41.101442	1770.110555	17.841639
41.309991	1762.667525	17.846656
41.460077	1754.305708	17.851674
41.245582	1761.347403	17.856691
41.104902	1761.984340	17.861709
41.483915	1767.211223	17.866727
41.386444	1766.132907	17.871744
41.250245	1752.624804	17.876762
41.395588	1758.806055	17.881779
41.486582	1762.738609	17.886797
41.357797	1758.839253	17.891815
41.710826	1767.882634	17.896832
41.674147	1756.837041	17.901850
41.349088	1763.435458	17.906867
41.899930	1763.326587	17.911885
41.817940	1771.894276	17.916903
41.769766	1778.266852	17.921920
42.202762	1764.230646	17.926938
41.815997	1761.335156	17.931955
41.946441	1756.989391	17.936973
41.712345	1763.076996	17.941991
41.848671	1762.078587	17.947008
42.115040	1747.948631	17.952026
41.848774	1762.320467	17.957043
41.962988	1771.530143	17.962061
42.155381	1768.951287	17.967079
42.359452	1781.781237	17.972096
42.532443	1771.819867	17.977114
42.132127	1760.030782	17.982131
42.145052	1751.067115	17.987149
42.208768	1765.682068	17.992167
42.191923	1777.302941	17.997184
42.050819	1782.260410	18.002202
41.954349	1795.602361	18.007219
42.130751	1791.505668	18.012237
42.302866	1782.871324	18.017255
41.988765	1793.706672	18.022272
42.205846	1781.919782	18.027290
42.663270	1794.626752	18.032307
42.572498	1806.691249	18.037325
42.759874	1808.037241	18.042343
42.889908	1806.765330	18.047360
43.048489	1801.474362	18.052378
43.195484	1806.380386	18.057395
42.654887	1795.034444	18.062413
42.936314	1783.837421	18.067431
42.890834	1786.125855	18.072448
43.162859	1778.141779	18.077466
42.740847	1779.606978	18.082483
42.942325	1795.140691	18.087501
43.309097	1804.209432	18.092519
43.209662	1808.556200	18.097536
43.229340	1804.073924	18.102554
43.380019	1808.303723	18.107571
43.332320	1810.276325	18.112589
43.369143	1801.884565	18.117607
43.376384	1796.629532	18.122624
43.448185	1792.864137	18.127642
43.192073	1790.620297	18.132659
43.607377	1792.362534	18.137677
43.520144	1797.839185	18.142695
43.133869	1804.004561	18.147712
43.978660	1796.223297	18.152730
43.512592	1806.811533	18.157747
43.756760	1803.028872	18.162765
43.346339	1796.736931	18.167783
43.491330	1808.359548	18.172800
43.324449	1804.555135	18.177818
43.499957	1800.589935	18.182835
43.391368	1800.416338	18.187853
43.552014	1803.029777	18.192871
43.613361	1800.392374	18.197888
43.731171	1816.416884	18.202906
44.143853	1835.620782	18.207923
44.146519	1829.940947	18.212941
44.098680	1832.125154	18.217959
44.095489	1834.094594	18.222976
44.204966	1819.833067	18.227994
44.197387	1828.451060	18.233011
44.384306	1828.039991	18.238029
44.221202	1816.059653	18.243047
44.075776	1823.882410	18.248064
44.500380	1811.537777	18.253082
44.382873	1816.294072	18.258099
44.599828	1820.642298	18.263117
44.511556	1821.560327	18.268135
44.602371	1817.186256	18.273152
44.764000	1815.861327	18.278170
44.486732	1818.696410	18.283187
44.633785	1817.387963	18.288205
44.855366	1806.144623	18.293223
44.651845	1819.846602	18.298240
44.764692	1812.741291	18.303258
44.720833	1807.669016	18.308275
44.574049	1821.228235	18.313293
45.056000	1798.010753	18.318311
44.718617	1806.104796	18.323328
44.894450	1810.232266	18.328346
44.786566	1812.666728	18.333363
44.597340	1810.839309	18.338381
45.055894	1829.202150	18.343399
44.797969	1839.510241	18.348416
45.266227	1835.815320	18.353434
45.319323	1834.644557	18.358451
45.026177	1843.145286	18.363469
45.531662	1840.671435	18.368487
45.687892	1846.301979	18.373504
45.575183	1831.525295	18.378522
45.487305	1837.976590	18.383539
45.283185	1841.549588	18.388557
45.597540	1839.320158	18.393575
45.628241	1836.527182	18.398592
45.333227	1842.951736	18.403610
45.815908	1848.058293	18.408627
45.314618	1844.571479	18.413645
45.384525	1828.964973	18.418663
45.375915	1841.595292	18.423680
45.470171	1836.913128	18.428698
45.454347	1859.247408	18.433715
45.903721	1871.908538	18.438733
46.054934	1871.654965	18.443751
45.252379	1866.087016	18.448768
45.617785	1876.010208	18.453786
46.108388	1859.305415	18.458803
45.898570	1880.092072	18.463821
45.970309	1869.066857	18.468839
46.049175	1870.537131	18.473856
46.016997	1873.513257	18.478874
46.177903	1880.643010	18.483891
46.213095	1893.114584	18.488909
46.449318	1897.698870	18.493927
46.480288	1893.272184	18.498944
46.437401	1898.987990	18.503962
46.673144	1889.586778	18.508979
46.643702	1898.226389	18.513997
46.670815	1886.157453	18.519015
47.195740	1884.889415	18.524032
47.156927	1884.431757	18.529050
47.143927	1859.575297	18.534067
46.796307	1852.521380	18.539085
47.114458	1849.449741	18.544103
46.840303	1858.595563	18.549120
46.685115	1853.006177	18.554138
47.045644	1843.350704	18.559155
47.093247	1854.182683	18.564173
47.168393	1842.900531	18.569191
47.233869	1854.851271	18.574208
47.204493	1840.095109	18.579226
46.867938	1844.474985	18.584243
46.793371	1849.147361	18.589261
47.046964	1856.840431	18.594279
47.062608	1870.730883	18.599296
47.361338	1883.600099	18.604314
47.240616	1873.604487	18.609331
47.076811	1876.167432	18.614349
47.362089	1879.992739	18.619367
47.525760	1884.160711	18.624384
47.577325	1880.407959	18.629402
47.842647	1870.331906	18.634419
47.586513	1879.144518	18.639437
47.731158	1872.907172	18.644455
47.471466	1868.719552	18.649472
47.507908	1891.558374	18.654490
47.895810	1873.534389	18.659507
47.492421	1867.603106	18.664525
47.663028	1896.819081	18.669543
47.886560	1904.697876	18.674560
48.059575	1908.195800	18.679578
48.059795	1904.997094	18.684595
47.510252	1909.625683	18.689613
47.804808	1905.525847	18.694631
48.004675	1911.251709	18.699648
48.143143	1903.339204	18.704666
47.877542	1905.651750	18.709683
47.820039	1911.441467	18.714701
48.364388	1923.662760	18.719719
48.522471	1938.752856	18.724736
48.357935	1939.968571	18.729754
48.657635	1940.337074	18.734771
48.478945	1950.736431	18.739789
48.607298	1936.081652	18.744807
48.849626	1933.874707	18.749824
48.500792	1939.687300	18.754842
48.566676	1933.855764	18.759859
48.678931	1926.426435	18.764877
48.826874	1931.133354	18.769895
48.469502	1931.491023	18.774912
48.956566	1933.652077	18.779930
49.104390	1926.278426	18.784947
48.974526	1936.262555	18.789965
49.334744	1922.182746	18.794983
49.090675	1931.102009	18.800000
49.171817	1925.448948	18.805018
49.347218	1926.560111	18.810035
49.264532	1926.367437	18.815053
49.422431	1928.251421	18.820071
49.286266	1925.713138	18.825088
49.072274	1928.295108	18.830106
49.426818	1924.038615	18.835123
49.394198	1928.909616	18.840141
49.459417	1924.086544	18.845159
49.442293	1928.773381	18.850176
49.337881	1928.395400	18.855194
49.590788	1928.551918	18.860211
49.490182	1929.762943	18.865229
49.640197	1946.044381	18.870247
49.670400	1945.231993	18.875264
49.993047	1953.750203	18.880282
50.058043	1948.039144	18.885299
49.879749	1954.158042	18.890317
49.965568	1950.002603	18.895335
49.983026	1951.336380	18.900352
50.184801	1950.498203	18.905370
50.285653	1951.765981	18.910387
50.372013	1954.146679	18.915405
50.214589	1949.486526	18.920423
50.357713	1951.689063	18.925440
50.486570	1949.758986	18.930458
50.535643	1948.556607	18.935475
50.271466	1947.478120	18.940493
50.490533	1941.285508	18.945511
50.827352	1943.046574	18.950528
50.669160	1942.002311	18.955546
50.683365	1922.516679	18.960563
50.410228	1925.204039	18.965581
50.578776	1940.381348	18.970599
50.600883	1950.610249	18.975616
50.147856	1951.215206	18.980634
50.295941	1947.126133	18.985651
50.396506	1945.149443	18.990669
50.281370	1952.434945	18.995687
50.587209	1955.768546	19.000704
50.676824	1980.193363	19.005722
51.065099	1976.331043	19.010739
50.945398	1983.176034	19.015757
51.233506	1983.952247	19.020775
51.421048	1978.933461	19.025792
51.443812	1977.133564	19.030810
51.619556	1972.825344	19.035827
51.274422	1988.961628	19.040845
51.380026	1983.030138	19.045863
51.717924	1967.219502	19.050880
51.445127	1979.198335	19.055898
51.242647	1987.629630	19.060915
51.322610	1976.407171	19.065933
51.109730	1967.491968	19.070951
51.174824	1975.119990	19.075968
51.282999	1982.457987	19.080986
51.330620	1992.039450	19.086003
51.620194	2001.629526	19.091021
51.916649	2008.153318	19.096039
51.970697	2007.996254	19.101056
51.899849	2000.899698	19.106074
52.015969	1997.426072	19.111091
51.871672	2005.979453	19.116109
51.798232	1997.905627	19.121127
51.710356	2004.346770	19.126144
51.974467	2005.928308	19.131162
52.034032	2024.387276	19.136179
52.309207	2022.691058	19.141197
52.246743	2026.187237	19.146215
52.779157	2016.058264	19.151232
52.514730	2017.802748	19.156250
52.613210	2023.892480	19.161267
52.594979	2022.900613	19.166285
52.531943	2021.131698	19.171303
52.593730	2019.058930	19.176320
52.812178	2021.166877	19.181338
53.264373	2009.972337	19.186355
53.298499	2005.670962	19.191373
53.167230	2011.647884	19.196391
53.368544	1994.350393	19.201408
53.232323	1985.760383	19.206426
53.290862	1982.477637	19.211443
53.214548	1986.113662	19.216461
53.064643	1989.674903	19.221479
53.326459	1984.927429	19.226496
53.247254	1978.230210	19.231514
53.177819	1983.704093	19.236531
53.156558	1988.528469	19.241549
53.039294	1976.965424	19.246567
53.427425	1984.366533	19.251584
53.219333	1975.547306	19.256602
53.030429	1978.117418	19.261619
53.063950	2005.385952	19.266637
53.281594	2007.484586	19.271655
53.272663	2005.889524	19.276672
53.221089	2013.728091	19.281690
53.868523	2003.441563	19.286707
53.673366	2020.388495	19.291725
53.349132	2012.205999	19.296743
53.988927	2033.113009	19.301760
53.907427	2033.570624	19.306778
54.038241	2049.525674	19.311795
54.125659	2058.890038	19.316813
53.919535	2048.313289	19.321831
53.788756	2049.868141	19.326848
53.723245	2059.205768	19.331866
53.880886	2054.131161	19.336883
54.054830	2047.651529	19.341901
54.081469	2055.920475	19.346919
54.559255	2046.420785	19.351936
54.371929	2050.275887	19.356954
54.200243	2069.669251	19.361971
54.682280	2070.895914	19.366989
54.043316	2072.418548	19.372007
54.790897	2063.667095	19.377024
54.299653	2082.917946	19.382042
54.566898	2073.626429	19.387059
54.406445	2074.775434	19.392077
54.291747	2083.843267	19.397095
54.532473	2091.436261	19.402112
54.793947	2095.793989	19.407130
55.074270	2098.568518	19.412147
55.257770	2105.814336	19.417165
55.232149	2108.660469	19.422183
55.367740	2098.988002	19.427200
55.195932	2098.947185	19.432218
55.499214	2103.720628	19.437235
55.683984	2091.876504	19.442253
55.554150	2098.128527	19.447271
55.827688	2091.566922	19.452288
55.617572	2100.522560	19.457306
55.613989	2095.727708	19.462323
55.906621	2085.986158	19.467341
55.751838	2095.706153	19.472359
55.500318	2066.851555	19.477376
55.494370	2088.936848	19.482394
55.721617	2093.657916	19.487411
56.110636	2094.823120	19.492429
55.877761	2099.023718	19.497447
55.998000	2095.446374	19.502464
55.803164	2093.510482	19.507482
55.851311	2092.488360	19.512499
56.015224	2090.175127	19.517517
55.748915	2094.762536	19.522535
56.065760	2092.476827	19.527552
56.119012	2104.563436	19.532570
56.074649	2091.666472	19.537587
56.673556	2108.331920	19.542605
56.517244	2111.786454	19.547623
56.536928	2097.487063	19.552640
56.045180	2094.195303	19.557658
56.325383	2111.868821	19.562675
56.631714	2119.384510	19.567693
56.155275	2130.907491	19.572711
56.711698	2121.208797	19.577728
56.543990	2118.631463	19.582746
56.426182	2134.861436	19.587763
56.421081	2118.879595	19.592781
56.881861	2152.325538	19.597799
57.171085	2139.167680	19.602816
57.068631	2151.752669	19.607834
57.284482	2156.579401	19.612851
57.301296	2142.949786	19.617869
57.161902	2156.327229	19.622887
57.353313	2146.686730	19.627904
57.386322	2142.851135	19.632922
57.480659	2150.319633	19.637939
57.729494	2141.956004	19.642957
57.609581	2145.434630	19.647975
57.527150	2153.429999	19.652992
57.425697	2159.594147	19.658010
57.489413	2150.923387	19.663027
57.522735	2146.614233	19.668045
57.581396	2141.924277	19.673063
58.040495	2132.554934	19.678080
57.827794	2144.196323	19.683098
57.555644	2142.913799	19.688115
57.944720	2140.320818	19.693133
58.266590	2141.464485	19.698151
58.194210	2141.587934	19.703168
57.872227	2139.786363	19.708186
58.007657	2154.885016	19.713203
58.010482	2150.189017	19.718221
57.784454	2162.403588	19.723239
58.073990	2154.907330	19.728256
58.214382	2160.035552	19.733274
58.231648	2167.791646	19.738291
58.291983	2164.244289	19.743309
58.060232	2176.547092	19.748327
58.406733	2177.155906	19.753344
58.907566	2180.579594	19.758362
58.669405	2190.331040	19.763379
58.872656	2186.049834	19.768397
58.747557	2186.348441	19.773415
58.786353	2179.878506	19.778432
59.310682	2188.168051	19.783450
58.796914	2186.344360	19.788467
59.119942	2177.153215	19.793485
59.276788	2183.101563	19.798503
59.255149	2177.460864	19.803520
58.923598	2182.797286	19.808538
58.811701	2176.580273	19.813555
59.274756	2182.068417	19.818573
59.099624	2212.807101	19.823591
59.050925	2206.476957	19.828608
59.115732	2216.998917	19.833626
59.277705	2207.822425	19.838643
59.923005	2206.944179	19.843661
59.658340	2200.446332	19.848679
59.909389	2212.031909	19.853696
59.909825	2203.599313	19.858714
59.838144	2201.435327	19.863731
60.071550	2200.515009	19.868749
59.647907	2206.823372	19.873767
59.958673	2206.403556	19.878784
59.996127	2209.323025	19.883802
59.927782	2213.141105	19.888819
60.198094	2218.838550	19.893837
60.247005	2226.470072	19.898855
60.394849	2227.668243	19.903872
60.566340	2228.595211	19.908890
60.418949	2233.239208	19.913907
60.834786	2226.898685	19.918925
60.718742	2225.735987	19.923943
60.826416	2230.167836	19.928960
60.806938	2221.253095	19.933978
61.045968	2224.076710	19.938995
60.961336	2212.106339	19.944013
60.676508	2204.272976	19.949031
61.146135	2214.528229	19.954048
61.316559	2212.169891	19.959066
60.986317	2193.442801	19.964083
61.092809	2199.664258	19.969101
60.973167	2212.536776	19.974119
61.286983	2208.727173	19.979136
61.340523	2214.252321	19.984154
61.213868	2231.619611	19.989171
61.456591	2222.716541	19.994189
61.394280	2219.843150	19.999207
61.413815	2226.616496	20.004224
61.702536	2221.592505	20.009242
61.413254	2226.636679	20.014259
61.605596	2219.271513	20.019277
61.564140	2226.491128	20.024295
61.760223	2222.041156	20.029312
61.523414	2217.474593	20.034330
61.475017	2219.268024	20.039347
61.575985	2241.217727	20.044365
61.929011	2247.894639	20.049383
61.979096	2248.844116	20.054400
62.057762	2256.763510	20.059418
62.121366	2256.849542	20.064435
62.109299	2245.288385	20.069453
62.009145	2259.288130	20.074471
62.332541	2254.455239	20.079488
62.298529	2244.263847	20.084506
62.136581	2261.151489	20.089523
62.323321	2252.465769	20.094541
62.524853	2270.418672	20.099559
62.556761	2276.837687	20.104576
62.593193	2276.401053	20.109594
62.142204	2287.343543	20.114611
62.613825	2282.324186	20.119629
62.426560	2283.616704	20.124647
62.511206	2282.475482	20.129664
62.805171	2297.713394	20.134682
62.707113	2308.536692	20.139699
62.991048	2300.958663	20.144717
63.074774	2313.473985	20.149735
63.296063	2310.076329	20.154752
63.169080	2302.187850	20.159770
63.034895	2306.437267	20.164787
63.796727	2298.241082	20.169805
63.589286	2304.350616	20.174823
63.430266	2297.180666	20.179840
63.965275	2291.769712	20.184858
63.723578	2300.732868	20.189875
63.821787	2297.435859	20.194893
63.678124	2298.879526	20.199911
63.892767	2296.967973	20.204928
63.870658	2295.718711	20.209946
63.960489	2302.663365	20.214963
64.093845	2284.126513	20.219981
64.259953	2303.028200	20.224999
63.892578	2295.181207	20.230016
64.449078	2308.712886	20.235034
64.362741	2328.750554	20.240051
64.498203	2320.513450	20.245069
64.859928	2327.509932	20.250087
64.742730	2310.923579	20.255104
64.892930	2292.617641	20.260122
64.254064	2295.144725	20.265139
64.627971	2280.003671	20.270157
64.720244	2294.285030	20.275175
64.485615	2301.121753	20.280192
64.872943	2313.470674	20.285210
64.677018	2326.653567	20.290227
64.584086	2321.124075	20.295245
64.673212	2324.232756	20.300263
64.691344	2329.453686	20.305280
64.746694	2319.974780	20.310298
64.678396	2338.432513	20.315315
65.214657	2325.000695	20.320333
65.264974	2345.221101	20.325351
65.081661	2352.781962	20.330368
65.385009	2340.323293	20.335386
65.081158	2353.941877	20.340403
65.421941	2336.263850	20.345421
65.530111	2358.343152	20.350439
65.769343	2370.682703	20.355456
66.270423	2363.965132	20.360474
66.026486	2357.924052	20.365491
66.042425	2344.395069	20.370509
65.943884	2342.457944	20.375527
65.981603	2349.883660	20.380544
66.057264	2341.513712	20.385562
65.539948	2357.287721	20.390579
65.676661	2363.096199	20.395597
65.924957	2370.286982	20.400615
66.014716	2377.343377	20.405632
66.233864	2373.518153	20.410650
66.166159	2373.909079	20.415667
66.427392	2381.119828	20.420685
66.666838	2382.102042	20.425703
66.668711	2397.241910	20.430720
66.810860	2398.496064	20.435738
66.553433	2404.307633	20.440755
66.816970	2399.444126	20.445773
67.053851	2407.993587	20.450791
66.722376	2414.409259	20.455808
66.677546	2399.760395	20.460826
66.753191	2417.167222	20.465843
66.874881	2396.690036	20.470861
67.028758	2402.246449	20.475879
66.725658	2408.589161	20.480896
67.287365	2414.248868	20.485914
67.418991	2433.899535	20.490931
67.418920	2432.366726	20.495949
67.590420	2433.294493	20.500967
67.457108	2432.536472	20.505984
67.874131	2433.015279	20.511002
67.622060	2430.709339	20.516019
67.764822	2435.938748	20.521037
67.913397	2425.006262	20.526055
67.449169	2436.359205	20.531072
67.697659	2427.320588	20.536090
67.496950	2437.935391	20.541107
67.644045	2453.768728	20.546125
68.010029	2456.779013	20.551143
68.047695	2454.475631	20.556160
68.448432	2446.523369	20.561178
68.372942	2457.481615	20.566195
68.309477	2440.410667	20.571213
68.658268	2448.626103	20.576231
68.445080	2449.943220	20.581248
68.923015	2442.747920	20.586266
68.536923	2447.299479	20.591283
68.821190	2472.345366	20.596301
68.882470	2469.825840	20.601319
68.970474	2477.092580	20.606336
69.177669	2471.764514	20.611354
69.122299	2485.345954	20.616371
69.294045	2471.189488	20.621389
69.429788	2472.343201	20.626407
69.169422	2466.659442	20.631424
69.480304	2480.812519	20.636442
69.465859	2476.532909	20.641459
69.456244	2456.350308	20.646477
69.132177	2462.571321	20.651495
69.450341	2465.691488	20.656512
69.528925	2456.574547	20.661530
69.597387	2471.377444	20.666547
69.584237	2462.682574	20.671565
69.835017	2462.441433	20.676583
69.913209	2462.503116	20.681600
69.930639	2466.335899	20.686618
70.176657	2465.953147	20.691635
69.939393	2463.279081	20.696653
69.914872	2464.454419	20.701671
69.867638	2469.387711	20.706688
70.292278	2459.563509	20.711706
69.982470	2478.510642	20.716723
70.024757	2501.089917	20.721741
70.278199	2491.913606	20.726759
70.154081	2495.614014	20.731776
70.317794	2489.951501	20.736794
70.453796	2499.298962	20.741811
70.433075	2494.717515	20.746829
70.798354	2512.296150	20.751847
70.387097	2525.536371	20.756864
70.705913	2514.184952	20.761882
70.956679	2523.779205	20.766899
71.028776	2528.171198	20.771917
71.042355	2516.991160	20.776935
70.904632	2533.947619	20.781952
71.166437	2537.853145	20.786970
71.578351	2538.733141	20.791987
71.380008	2555.565574	20.797005
71.487039	2537.684675	20.802023
71.622096	2548.463895	20.807040
71.827923	2548.893796	20.812058
71.808071	2554.032767	20.817075
71.666493	2547.397934	20.822093
72.216164	2548.026281	20.827111
71.654926	2539.566647	20.832128
71.990172	2541.340627	20.837146
72.132067	2539.308499	20.842163
71.793005	2538.808245	20.847181
72.349078	2533.416655	20.852199
71.981030	2541.270577	20.857216
72.062975	2534.419978	20.862234
72.276043	2533.690090	20.867251
72.382852	2562.746103	20.872269
72.555417	2560.844374	20.877287
72.309315	2577.685235	20.882304
72.551586	2574.402160	20.887322
72.819133	2568.387188	20.892339
72.729788	2575.808112	20.897357
72.862174	2569.790309	20.902375
72.573589	2567.609729	20.907392
72.799351	2556.233001	20.912410
73.216844	2551.118358	20.917427
72.521354	2574.384098	20.922445
73.130368	2579.529768	20.927463
73.051280	2594.709496	20.932480
73.234834	2594.553012	20.937498
73.464770	2594.021798	20.942515
73.436785	2584.503308	20.947533
73.486459	2588.534707	20.952551
73.461915	2588.518384	20.957568
73.271507	2592.098028	20.962586
73.653269	2584.713484	20.967603
73.530488	2607.231937	20.972621
73.966878	2615.184938	20.977639
73.772580	2619.751586	20.982656
73.916161	2617.620069	20.987674
73.952050	2610.654858	20.992691
74.078440	2621.080765	20.997709
74.444924	2607.417765	21.002727
74.057870	2613.401898	21.007744
74.323667	2616.173340	21.012762
74.519740	2603.183306	21.017779
74.301389	2618.441114	21.022797
74.657475	2624.212353	21.027815
74.893979	2632.126446	21.032832
75.075540	2637.446492	21.037850
75.028041	2626.836946	21.042867
75.020321	2631.986595	21.047885
75.366868	2627.688703	21.052903
75.296740	2625.610929	21.057920
75.279408	2610.988145	21.062938
75.561096	2598.270778	21.067955
75.419749	2601.089839	21.072973
75.577353	2576.488906	21.077991
75.569374	2591.842139	21.083008
75.314933	2591.876636	21.088026
75.577309	2594.931790	21.093043
75.565267	2616.439928	21.098061
75.617652	2615.139430	21.103079
75.648428	2629.410473	21.108096
75.435079	2626.048234	21.113114
76.172949	2610.118061	21.118131
75.856402	2630.672671	21.123149
76.106488	2621.690314	21.128167
76.110845	2635.521156	21.133184
75.875958	2620.645164	21.138202
76.149886	2629.497977	21.143219
76.375434	2651.563725	21.148237
76.304131	2646.361027	21.153255
76.184073	2651.260371	21.158272
76.418475	2653.779613	21.163290
76.791883	2645.577534	21.168307
76.648604	2647.642576	21.173325
76.781601	2650.515434	21.178343
76.986489	2638.891050	21.183360
76.602234	2654.113211	21.188378
76.840957	2643.954346	21.193395
76.951189	2671.510009	21.198413
77.151300	2664.670396	21.203431
77.035668	2687.388411	21.208448
76.963007	2684.243633	21.213466
77.198370	2675.497994	21.218483
77.005899	2682.194451	21.223501
77.180070	2680.320768	21.228519
77.205618	2684.118490	21.233536
77.647920	2706.432928	21.238554
77.955407	2697.556213	21.243571
77.799791	2709.728548	21.248589
77.982669	2705.701363	21.253607
77.821552	2705.359933	21.258624
77.713911	2711.063571	21.263642
78.162284	2710.693380	21.268659
78.102141	2702.068789	21.273677
78.176869	2707.385445	21.278695
77.811150	2700.649418	21.283712
78.219651	2717.768335	21.288730
78.425979	2728.492275	21.293747
78.709990	2731.886175	21.298765
78.563219	2723.297410	21.303783
78.560792	2731.465185	21.308800
78.659609	2723.584519	21.313818
79.355968	2720.295861	21.318835
78.867214	2724.601154	21.323853
79.224981	2727.844851	21.328871
79.394092	2725.057164	21.333888
79.153179	2720.527277	21.338906
79.541042	2721.094913	21.343923
79.190979	2728.648735	21.348941
79.063562	2722.619598	21.353959
79.597136	2740.325844	21.358976
79.357184	2750.282460	21.363994
79.702557	2752.684127	21.369011
79.551905	2757.331956	21.374029
79.396014	2755.200979	21.379047
79.633355	2756.954417	21.384064
79.700043	2743.796108	21.389082
79.739173	2749.090140	21.394099
79.784016	2760.445531	21.399117
80.383203	2765.815442	21.404135
80.443377	2773.563443	21.409152
80.588835	2775.956877	21.414170
80.955074	2767.596983	21.419187
80.750090	2768.717743	21.424205
80.506390	2775.764580	21.429223
80.702067	2776.878084	21.434240
80.719233	2779.886642	21.439258
80.916957	2770.540486	21.444275
80.748313	2774.239411	21.449293
80.985664	2767.397744	21.454311
80.859220	2767.250578	21.459328
80.874542	2776.732305	21.464346
80.858141	2764.376181	21.469363
80.625601	2779.040968	21.474381
81.233193	2780.267342	21.479399
81.156203	2792.262023	21.484416
81.166278	2790.071538	21.489434
81.538468	2789.866094	21.494451
81.335120	2804.449952	21.499469
81.607528	2794.774872	21.504487
81.768063	2802.533629	21.509504
81.335455	2807.602428	21.514522
82.031261	2812.530616	21.519539
81.643983	2829.858370	21.524557
81.627405	2831.259797	21.529575
82.039189	2822.574823	21.534592
81.872354	2839.474138	21.539610
82.026770	2843.014586	21.544627
82.219259	2864.903438	21.549645
82.342140	2857.357886	21.554663
82.809941	2857.008193	21.559680
82.797254	2856.193156	21.564698
82.956636	2852.211367	21.569715
83.235188	2845.496029	21.574733
83.018643	2850.636579	21.579751
83.264923	2838.857556	21.584768
83.188076	2848.180189	21.589786
83.193236	2838.719963	21.594803
83.270128	2854.253440	21.599821
83.456400	2838.963174	21.604839
83.382805	2848.264051	21.609856
83.266551	2846.162924	21.614874
83.281273	2843.065531	21.619891
83.655855	2850.282825	21.624909
83.591340	2865.447924	21.629927
83.990398	2868.696082	21.634944
84.063200	2865.897768	21.639962
84.369112	2855.750854	21.644979
84.063673	2872.935820	21.649997
84.103622	2863.501494	21.655015
84.417380	2862.315040	21.660032
84.320847	2865.897872	21.665050
84.325590	2866.882151	21.670067
84.498839	2863.967136	21.675085
84.357189	2866.003630	21.680103
84.597806	2856.676537	21.685120
84.448520	2864.151214	21.690138
84.523756	2858.892822	21.695155
84.638857	2872.948500	21.700173
84.896770	2886.472489	21.705191
85.071983	2889.167971	21.710208
84.896780	2890.533344	21.715226
85.292747	2894.790422	21.720243
85.359061	2884.654164	21.725261
85.121705	2888.209115	21.730279
85.377947	2879.736122	21.735296
85.220198	2895.126928	21.740314
85.229572	2874.377514	21.745331
85.443007	2897.651423	21.750349
85.561262	2906.931183	21.755367
85.724761	2915.111146	21.760384
85.638612	2916.451307	21.765402
85.833497	2906.511633	21.770419
85.714278	2921.163997	21.775437
85.860671	2909.886179	21.780455
85.923247	2926.262891	21.785472
86.197589	2934.520368	21.790490
86.136630	2943.070445	21.795507
86.370267	2935.739239	21.800525
86.553072	2944.104136	21.805543
86.395239	2935.091458	21.810560
86.272011	2944.780240	21.815578
86.773923	2946.729852	21.820595
86.861387	2962.191750	21.825613
86.624452	2954.066378	21.830631
87.054848	2961.355847	21.835648
87.077089	2971.394299	21.840666
87.432611	2954.771161	21.845683
87.191841	2962.265197	21.850701
86.962290	2956.442608	21.855719
87.359725	2971.975437	21.860736
87.384841	2977.657222	21.865754
87.627237	2982.812733	21.870771
87.767360	2978.584628	21.875789
87.680508	2990.798147	21.880807
87.756607	2983.009063	21.885824
87.907487	2994.369752	21.890842
87.854747	2985.560534	21.895859
88.164320	2996.859735	21.900877
87.969664	2997.031793	21.905895
88.686414	3010.753322	21.910912
88.482170	3014.412361	21.915930
88.770875	3005.822421	21.920947
89.025216	3006.374392	21.925965
88.967844	3009.486916	21.930983
89.097592	3001.357320	21.936000
88.983959	3012.448707	21.941018
89.000865	2996.230346	21.946035
89.109470	2994.379665	21.951053
89.024677	3001.020552	21.956071
89.394250	2998.681463	21.961088
89.159014	3000.239698	21.966106
89.375761	2993.977007	21.971123
89.304625	2999.547506	21.976141
89.483480	2989.375924	21.981159
89.466983	2993.105704	21.986176
89.689117	3013.022753	21.991194
89.828383	3022.361378	21.996211
89.759441	3022.154696	22.001229
89.713124	3034.272113	22.006247
90.131815	3024.971580	22.011264
89.820720	3027.404035	22.016282
89.772032	3029.624739	22.021299
90.275777	3030.044908	22.026317
90.242111	3046.297086	22.031335
90.658609	3041.548207	22.036352
90.583466	3044.603003	22.041370
90.927961	3039.794812	22.046387
91.199301	3046.485122	22.051405
90.741897	3049.830566	22.056423
91.262582	3039.306315	22.061440
91.245450	3030.508697	22.066458
91.031111	3034.740427	22.071475
91.575947	3031.777924	22.076493
91.280923	3041.744306	22.081511
91.836037	3025.665844	22.086528
91.316262	3036.429497	22.091546
91.692541	3038.657165	22.096563
91.696148	3032.777699	22.101581
91.561885	3038.328388	22.106599
91.862262	3029.233931	22.111616
91.808824	3033.743634	22.116634
91.669746	3031.871875	22.121651
91.768428	3015.623933	22.126669
92.146010	3028.145714	22.131687
92.099449	3049.217922	22.136704
91.996555	3057.524611	22.141722
92.300473	3055.331280	22.146739
92.435335	3049.269623	22.151757
92.364039	3053.854548	22.156775
92.384580	3065.243156	22.161792
92.606056	3066.540570	22.166810
92.459055	3085.258005	22.171827
92.672275	3078.215524	22.176845
92.691654	3092.591097	22.181863
92.960988	3079.022599	22.186880
93.117667	3096.325283	22.191898
92.958151	3108.247641	22.196915
93.314734	3104.756649	22.201933
93.327764	3117.714999	22.206951
93.317543	3120.520328	22.211968
93.597934	3113.504089	22.216986
93.719452	3122.757509	22.222003
94.134239	3139.014581	22.227021
93.914732	3143.709695	22.232039
94.153356	3134.975063	22.237056
94.104436	3149.809166	22.242074
94.028682	3145.202465	22.247091
94.349598	3145.470871	22.252109
94.497725	3145.069891	22.257127
94.353034	3138.207165	22.262144
94.280391	3139.925127	22.267162
94.393305	3153.629023	22.272179
94.616959	3166.351670	22.277197
94.830237	3165.357418	22.282215
95.044926	3159.774620	22.287232
94.982243	3172.156704	22.292250
94.903246	3163.877810	22.297267
95.346364	3155.611631	22.302285
95.198136	3171.278883	22.307303
95.702375	3153.809794	22.312320
95.418147	3170.708545	22.317338
95.338832	3176.402340	22.322355
95.684295	3184.863365	22.327373
95.869522	3194.485819	22.332391
95.822821	3191.237677	22.337408
96.053000	3190.396479	22.342426
95.687406	3187.074903	22.347443
96.321291	3185.363049	22.352461
96.088780	3186.452831	22.357479
96.156908	3180.935087	22.362496
96.241789	3181.922341	22.367514
96.236906	3208.530625	22.372531
96.532426	3216.622843	22.377549
96.575088	3217.799327	22.382567
96.673027	3214.948169	22.387584
96.962922	3214.393215	22.392602
96.508180	3217.355188	22.397619
97.006849	3223.051230	22.402637
96.911923	3236.450887	22.407655
97.005086	3249.421747	22.412672
97.380156	3240.015548	22.417690
97.243240	3243.444441	22.422707
97.204718	3252.334872	22.427725
97.303954	3256.104475	22.432743
97.751560	3265.582877	22.437760
98.044914	3280.640997	22.442778
98.160067	3275.013458	22.447795
98.319797	3259.493361	22.452813
98.233135	3267.729144	22.457831
98.113415	3269.633978	22.462848
98.439288	3266.087276	22.467866
98.173798	3277.889798	22.472883
98.375413	3263.913447	22.477901
98.631776	3266.335689	22.482919
98.523738	3277.523139	22.487936
98.998433	3285.212392	22.492954
98.787217	3285.918848	22.497971
99.150586	3283.210207	22.502989
98.909912	3288.074719	22.508007
98.873816	3287.156410	22.513024
99.322160	3278.351280	22.518042
99.100134	3289.303624	22.523059
99.511693	3306.799540	22.528077
99.449469	3304.991793	22.533095
99.856636	3304.610859	22.538112
99.750365	3313.119607	22.543130
99.706024	3316.106618	22.548147
100.161317	3307.817961	22.553165
99.956016	3309.372240	22.558183
100.420892	3313.548447	22.563200
100.190060	3308.403988	22.568218
100.339103	3294.359688	22.573235
100.478777	3304.323793	22.578253
100.293632	3317.041749	22.583271
100.432129	3320.203342	22.588288
100.945070	3320.244477	22.593306
100.807931	3341.176583	22.598323
101.005590	3327.067863	22.603341
101.120375	3325.681050	22.608359
100.728071	3322.329089	22.613376
100.947318	3324.573190	22.618394
100.942368	3332.884083	22.623411
101.356720	3340.022912	22.628429
101.142671	3345.017710	22.633447
101.324171	3357.844001	22.638464
101.687871	3348.511916	22.643482
101.335436	3357.118152	22.648499
101.694642	3347.233787	22.653517
101.788939	3360.944779	22.658535
101.932519	3389.524600	22.663552
102.357209	3381.004794	22.668570
102.329207	3384.993736	22.673587
102.354446	3373.321902	22.678605
102.412684	3381.566109	22.683623
102.556620	3383.849760	22.688640
102.787816	3371.672323	22.693658
102.670053	3371.832122	22.698675
103.063899	3395.330565	22.703693
103.144361	3393.207429	22.708711
103.241938	3408.084510	22.713728
103.307426	3401.664842	22.718746
103.345298	3397.837583	22.723763
103.505853	3409.285942	22.728781
103.333806	3399.698644	22.733799
103.451592	3403.580961	22.738816
103.775172	3405.981496	22.743834
103.563568	3407.264617	22.748851
103.467697	3406.144228	22.753869
103.491975	3427.820827	22.758887
103.851913	3437.689331	22.763904
104.036354	3431.346650	22.768922
103.904477	3440.623371	22.773939
104.525867	3454.223657	22.778957
104.694996	3458.817568	22.783975
104.435986	3458.331255	22.788992
104.991287	3448.184285	22.794010
104.822450	3471.754482	22.799027
104.946201	3454.334696	22.804045
105.223225	3458.589671	22.809063
105.055602	3459.469321	22.814080
105.047828	3456.112651	22.819098
104.954881	3476.318923	22.824115
105.196921	3478.383208	22.829133
105.435753	3486.535748	22.834151
105.216815	3498.926504	22.839168
105.384651	3479.722656	22.844186
105.470507	3506.228123	22.849203
105.603975	3514.564244	22.854221
105.783601	3519.201339	22.859239
105.874373	3516.178993	22.864256
106.100660	3507.768628	22.869274
106.504933	3520.391200	22.874291
106.026928	3507.031153	22.879309
106.308686	3523.743303	22.884327
106.591586	3531.366515	22.889344
107.078796	3533.630851	22.894362
106.961811	3546.097426	22.899379
106.984320	3537.336447	22.904397
107.040682	3541.068122	22.909415
107.057691	3533.280302	22.914432
107.285842	3530.635658	22.919450
107.414903	3540.744784	22.924467
107.656456	3531.287321	22.929485
107.702032	3523.149619	22.934503
107.753689	3526.649197	22.939520
107.813002	3536.948795	22.944538
107.781908	3554.206446	22.949555
108.107485	3568.316550	22.954573
108.170341	3556.074554	22.959591
108.377816	3555.321914	22.964608
108.350563	3558.172521	22.969626
108.131938	3560.270156	22.974643
108.495190	3561.456119	22.979661
108.496849	3560.980154	22.984679
108.546633	3584.492073	22.989696
108.967225	3574.852638	22.994714
109.174594	3591.435133	22.999731
109.061881	3580.253967	23.004749
109.203786	3585.626311	23.009767
109.365890	3584.926529	23.014784
109.353273	3581.547790	23.019802
109.545192	3594.552767	23.024819
109.501693	3583.993806	23.029837
109.676813	3581.972758	23.034855
109.397917	3606.693478	23.039872
109.550897	3606.326325	23.044890
109.862462	3609.780546	23.049907
110.083289	3603.520094	23.054925
109.683004	3604.860063	23.059943
109.939297	3622.141192	23.064960
110.308150	3636.929625	23.069978
110.276831	3653.300098	23.074995
110.292445	3631.680164	23.080013
110.876378	3654.241719	23.085031
110.798988	3660.684277	23.090048
111.293222	3663.369154	23.095066
111.136955	3650.711274	23.100083
111.280008	3669.066975	23.105101
111.507174	3650.751787	23.110119
111.575637	3659.457852	23.115136
111.870811	3646.047547	23.120154
111.555364	3656.222913	23.125171
111.708074	3656.268001	23.130189
112.098137	3649.967171	23.135207
111.764934	3656.377360	23.140224
112.069243	3646.300956	23.145242
111.878076	3655.852364	23.150259
111.637039	3673.498407	23.155277
112.116166	3672.091225	23.160295
112.074824	3666.847985	23.165312
112.210705	3671.539303	23.170330
112.450741	3695.060395	23.175347
112.670578	3707.478906	23.180365
112.803387	3693.518624	23.185383
112.715155	3700.440421	23.190400
113.354034	3691.286862	23.195418
113.386535	3701.735594	23.200435
113.124036	3704.054211	23.205453
113.722248	3708.680474	23.210471
113.317062	3727.243235	23.215488
113.545214	3731.972564	23.220506
113.775529	3728.518082	23.225523
113.371294	3722.332862	23.230541
113.941465	3720.379387	23.235559
113.994862	3753.140367	23.240576
114.184780	3740.974714	23.245594
114.448036	3752.626441	23.250611
114.185017	3749.597529	23.255629
114.396078	3749.558583	23.260647
114.826579	3756.827201	23.265664
114.913419	3763.452865	23.270682
114.963665	3766.642000	23.275699
115.047401	3781.649891	23.280717
115.163091	3762.963735	23.285735
115.301830	3768.235960	23.290752
115.307555	3768.958977	23.295770
115.856235	3766.458271	23.300787
115.752718	3769.549207	23.305805
115.904284	3757.841191	23.310823
115.700313	3769.609911	23.315840
115.746534	3777.672182	23.320858
115.896059	3797.270701	23.325875
115.772486	3800.081649	23.330893
116.211398	3792.159553	23.335911
115.972930	3800.994881	23.340928
115.827978	3815.344662	23.345946
116.520159	3817.456791	23.350963
116.443977	3828.197484	23.355981
116.541224	3831.322499	23.360999
116.932705	3833.935689	23.366016
117.452891	3853.763882	23.371034
117.570473	3845.707345	23.376051
117.681157	3849.328959	23.381069
117.990583	3848.693780	23.386087
117.919964	3851.005423	23.391104
117.928814	3839.633972	23.396122
118.241419	3828.048899	23.401139
118.118653	3812.459198	23.406157
118.212251	3808.848715	23.411175
118.306332	3803.278613	23.416192
118.286242	3797.726718	23.421210
118.458120	3810.450318	23.426227
118.282404	3822.338078	23.431245
118.768405	3836.313519	23.436263
118.590537	3846.555182	23.441280
118.415516	3835.309811	23.446298
118.914912	3831.445035	23.451315
118.859154	3836.999239	23.456333
118.987687	3833.207756	23.461351
118.909953	3843.844083	23.466368
118.863042	3849.489706	23.471386
119.468250	3868.088986	23.476403
118.930702	3865.135289	23.481421
119.464023	3865.074851	23.486439
119.422988	3899.844594	23.491456
119.426313	3895.617587	23.496474
119.660168	3910.124175	23.501491
119.779020	3906.279937	23.506509
119.977472	3917.997982	23.511527
120.027734	3928.526643	23.516544
120.123324	3935.392493	23.521562
120.523120	3942.598448	23.526579
120.458242	3950.929473	23.531597
120.763886	3957.260740	23.536615
120.638153	3955.977512	23.541632
120.951681	3957.723672	23.546650
121.416808	3977.580480	23.551667
121.241142	3989.387341	23.556685
121.278648	3981.214486	23.561703
121.684928	3988.414711	23.566720
121.847429	3979.776677	23.571738
121.807039	3982.899286	23.576755
121.815450	3986.914051	23.581773
121.999490	4002.072946	23.586791
122.152592	4008.902127	23.591808
122.265161	4002.313425	23.596826
122.640730	4013.112806	23.601843
122.610242	4002.460216	23.606861
122.599360	4007.490493	23.611879
122.698137	4010.759263	23.616896
122.887299	4025.517743	23.621914
123.483889	4028.989552	23.626931
123.399546	4028.781376	23.631949
123.534913	4034.268994	23.636967
123.438339	4021.923018	23.641984
123.264653	4036.860511	23.647002
123.728082	4021.272306	23.652019
123.224021	4031.345844	23.657037
123.370611	4029.643163	23.662055
123.753457	4052.730636	23.667072
123.858578	4062.334971	23.672090
123.950122	4056.935884	23.677107
123.918315	4056.867223	23.682125
124.635682	4069.955615	23.687143
124.927779	4077.197691	23.692160
124.853323	4080.409924	23.697178
125.008745	4071.462234	23.702195
125.029048	4080.768586	23.707213
125.298964	4068.869173	23.712231
125.047635	4079.991188	23.717248
124.921784	4076.425856	23.722266
125.161168	4067.848672	23.727283
125.124068	4091.747350	23.732301
125.500754	4098.414270	23.737319
125.459533	4111.382149	23.742336
125.245939	4113.175404	23.747354
125.724796	4123.293667	23.752371
125.933467	4131.810883	23.757389
126.451585	4127.838420	23.762407
126.087333	4138.300378	23.767424
126.015480	4141.248677	23.772442
126.788760	4148.152104	23.777459
126.629879	4159.052544	23.782477
126.704620	4153.351660	23.787495
126.866089	4157.327120	23.792512
126.696254	4171.328788	23.797530
127.098880	4180.411402	23.802547
127.278565	4175.188591	23.807565
127.718014	4181.234301	23.812583
127.553678	4185.676292	23.817600
127.358489	4196.380375	23.822618
127.942052	4195.084724	23.827635
128.364350	4198.901393	23.832653
128.366881	4209.373359	23.837671
128.717562	4207.609797	23.842688
128.651953	4212.135175	23.847706
128.933993	4192.917693	23.852723
129.122137	4201.873252	23.857741
128.919796	4201.329100	23.862759
129.149353	4191.702420	23.867776
128.812488	4208.504552	23.872794
129.131337	4198.538735	23.877811
129.305378	4205.553471	23.882829
129.243119	4214.818006	23.887847
129.247006	4225.687822	23.892864
129.247400	4227.129156	23.897882
129.265973	4232.922606	23.902899
129.574746	4261.535216	23.907917
129.935696	4256.484864	23.912935
130.207262	4273.998758	23.917952
130.105918	4263.964588	23.922970
130.698549	4269.802615	23.927987
130.188866	4287.127997	23.933005
130.431641	4286.921940	23.938023
130.935733	4279.691694	23.943040
130.792450	4289.034488	23.948058
131.191456	4285.217071	23.953075
131.114041	4285.546659	23.958093
130.977372	4297.136719	23.963111
131.241303	4300.457102	23.968128
131.149545	4315.156824	23.973146
131.537679	4305.732135	23.978163
131.538843	4324.407857	23.983181
131.803021	4343.305990	23.988199
132.074747	4329.910604	23.993216
132.026326	4329.248290	23.998234
132.413243	4333.939129	24.003251
132.684303	4327.689242	24.008269
132.728526	4335.107064	24.013287
133.036086	4325.084748	24.018304
132.767694	4343.633552	24.023322
133.418340	4333.975039	24.028339
133.426854	4353.783229	24.033357
133.503919	4361.742569	24.038375
133.450585	4356.254764	24.043392
133.333369	4361.678150	24.048410
133.423387	4352.464593	24.053427
133.545926	4357.775802	24.058445
133.555856	4352.128443	24.063463
134.132775	4356.032210	24.068480
134.129446	4383.970292	24.073498
134.436293	4368.898363	24.078515
134.368380	4378.138728	24.083533
134.310218	4381.192666	24.088551
134.763996	4386.418817	24.093568
135.016643	4395.807112	24.098586
135.067520	4412.773430	24.103603
135.234579	4415.656156	24.108621
135.115617	4409.000347	24.113639
135.446798	4400.002407	24.118656
135.216606	4414.649566	24.123674
135.528885	4408.526809	24.128691
135.523151	4427.840188	24.133709
135.332580	4431.530434	24.138727
135.875302	4436.956400	24.143744
135.644935	4440.826064	24.148762
136.079399	4453.240096	24.153779
136.105839	4472.881171	24.158797
136.364808	4467.785646	24.163815
136.728211	4467.635876	24.168832
136.793958	4482.931347	24.173850
136.745347	4482.554623	24.178867
137.432651	4479.954606	24.183885
137.102072	4490.880307	24.188903
137.491549	4478.219657	24.193920
136.989998	4489.318941	24.198938
137.315849	4496.992455	24.203955
137.372963	4519.233418	24.208973
137.821787	4509.898833	24.213991
137.960464	4507.940900	24.219008
138.080427	4539.244732	24.224026
138.325237	4537.204578	24.229043
138.628017	4539.351377	24.234061
138.466490	4540.743823	24.239079
138.605226	4526.428584	24.244096
138.560266	4536.467810	24.249114
138.880178	4523.700210	24.254131
139.054141	4555.390383	24.259149
138.839303	4557.806947	24.264167
139.392229	4553.929520	24.269184
139.580215	4563.148080	24.274202
139.498204	4558.163533	24.279219
140.104193	4551.189105	24.284237
139.584439	4573.904459	24.289255
140.011431	4573.119918	24.294272
140.212317	4579.971642	24.299290
140.121478	4585.909334	24.304307
139.973509	4588.841536	24.309325
140.221409	4591.939549	24.314343
141.038508	4612.330333	24.319360
140.498526	4617.836166	24.324378
140.639493	4618.547889	24.329395
141.216494	4621.148167	24.334413
141.194445	4641.870247	24.339431
141.146172	4637.297242	24.344448
141.330219	4643.899939	24.349466
141.335674	4648.714637	24.354483
141.587668	4656.657260	24.359501
141.579735	4668.260127	24.364519
141.837744	4673.224159	24.369536
141.849747	4676.707521	24.374554
142.381790	4697.128926	24.379571
142.709011	4696.612030	24.384589
142.626136	4701.521859	24.389607
142.720030	4695.034949	24.394624
142.718045	4719.711024	24.399642
143.004498	4719.617578	24.404659
143.511560	4739.861298	24.409677
143.368841	4726.243702	24.414695
143.542448	4711.859001	24.419712
143.658252	4720.026340	24.424730
143.567683	4741.501342	24.429747
143.962563	4745.222619	24.434765
144.092147	4754.596938	24.439783
144.279256	4747.977137	24.444800
144.238420	4752.992779	24.449818
144.346393	4764.438783	24.454835
144.838625	4771.576918	24.459853
144.672863	4787.963010	24.464871
145.216497	4776.116152	24.469888
144.998000	4787.741672	24.474906
145.081974	4774.201958	24.479923
145.483281	4785.368346	24.484941
144.999409	4800.309652	24.489959
145.285870	4805.118933	24.494976
145.423258	4805.125563	24.499994
145.811952	4818.227702	24.505011
146.107413	4824.126711	24.510029
146.022775	4829.251633	24.515047
146.725895	4817.486305	24.520064
146.467275	4832.232029	24.525082
146.293714	4822.394652	24.530099
146.515370	4832.146905	24.535117
146.961444	4847.884821	24.540135
147.117660	4856.176386	24.545152
147.265211	4860.419377	24.550170
147.152864	4863.354608	24.555187
147.437607	4852.369500	24.560205
147.418168	4867.909458	24.565223
147.619116	4873.456952	24.570240
147.724164	4884.429919	24.575258
147.740751	4885.876602	24.580275
147.911888	4891.194417	24.585293
148.173962	4898.607684	24.590311
148.450225	4900.473977	24.595328
148.336933	4913.428092	24.600346
148.337382	4919.694367	24.605363
148.899855	4928.406599	24.610381
148.730350	4950.457774	24.615399
149.269961	4941.050228	24.620416
149.622728	4948.481315	24.625434
149.566890	4962.726745	24.630451
150.110697	4955.557500	24.635469
149.769095	4965.959785	24.640487
149.872693	4965.634304	24.645504
150.007227	4961.384498	24.650522
150.071984	4968.374541	24.655539
150.535866	4968.192229	24.660557
150.279128	4989.892337	24.665575
150.742922	4984.936270	24.670592
151.203211	4988.975241	24.675610
151.040596	4990.765978	24.680627
151.531039	4987.155660	24.685645
151.489640	5004.064994	24.690663
151.632422	5020.449354	24.695680
151.769762	5024.219632	24.700698
151.994757	5014.202936	24.705715
152.250815	5020.927276	24.710733
151.656953	5022.107840	24.715751
152.218497	5007.709776	24.720768
152.624460	5009.401209	24.725786
152.529955	5041.740217	24.730803
152.912308	5030.124204	24.735821
152.742647	5032.771228	24.740839
152.968445	5041.172958	24.745856
152.728713	5034.643899	24.750874
153.021518	5040.910816	24.755891
153.662409	5057.226813	24.760909
153.541634	5064.333809	24.765927
153.682274	5059.426093	24.770944
153.847043	5065.814921	24.775962
153.662652	5069.918152	24.780979
154.008992	5074.833623	24.785997
153.795479	5091.156860	24.791015
154.400006	5091.405273	24.796032
153.977633	5094.102826	24.801050
154.388757	5112.524587	24.806067
154.637362	5115.823213	24.811085
154.357144	5121.550576	24.816103
154.732375	5145.275082	24.821120
155.227873	5151.206056	24.826138
154.993464	5161.147676	24.831155
155.082065	5168.827902	24.836173
155.502240	5185.812544	24.841191
155.598455	5177.048277	24.846208
155.862304	5194.067294	24.851226
155.722419	5223.990041	24.856243
156.301847	5209.516553	24.861261
156.169136	5217.524750	24.866279
156.503767	5241.419523	24.871296
156.686262	5225.863831	24.876314
156.720721	5249.317132	24.881331
157.256568	5248.117123	24.886349
157.483332	5269.792478	24.891367
157.564335	5276.716353	24.896384
157.644530	5266.457445	24.901402
157.799210	5270.960613	24.906419
158.259051	5256.082099	24.911437
158.450652	5286.862367	24.916455
158.524994	5294.062667	24.921472
158.733687	5278.084991	24.926490
158.672412	5289.520625	24.931507
159.182618	5289.141324	24.936525
159.420431	5275.674965	24.941543
159.428663	5284.873075	24.946560
159.493845	5272.821243	24.951578
159.474524	5286.953382	24.956595
159.495494	5276.852601	24.961613
159.508276	5298.791052	24.966631
159.672974	5307.753387	24.971648
159.971423	5305.492163	24.976666
159.910047	5321.988867	24.981683
160.346053	5327.282706	24.986701
160.284287	5329.643519	24.991719
159.949393	5338.432197	24.996736
160.525978	5345.474561	25.001754
160.720753	5362.859601	25.006771
161.149036	5365.133635	25.011789
161.102974	5370.697098	25.016807
160.813506	5370.784373	25.021824
161.637006	5384.130029	25.026842
161.403851	5392.153548	25.031859
161.472601	5404.148363	25.036877
161.799155	5423.122123	25.041895
161.974916	5427.597589	25.046912
161.981476	5425.831323	25.051930
162.007532	5432.566561	25.056947
162.315211	5444.553212	25.061965
162.835518	5454.662647	25.066983
162.775857	5447.697164	25.072000
163.071783	5460.314304	25.077018
163.059825	5471.879895	25.082035
163.350039	5473.518246	25.087053
163.705590	5474.335053	25.092071
163.940013	5468.470525	25.097088
164.365837	5481.848204	25.102106
164.304388	5494.770960	25.107123
164.674586	5494.260565	25.112141
164.677536	5499.190804	25.117159
164.519071	5508.167807	25.122176
164.743211	5489.661219	25.127194
164.880161	5497.724917	25.132211
164.911803	5502.132908	25.137229
165.241350	5519.039550	25.142247
165.331242	5526.001463	25.147264
165.338318	5521.000025	25.152282
165.370559	5534.317770	25.157299
166.157589	5536.696705	25.162317
165.922148	5546.946363	25.167335
165.943577	5557.011888	25.172352
166.098434	5542.855165	25.177370
166.380641	5575.044018	25.182387
166.548303	5584.436398	25.187405
166.830073	5579.245598	25.192423
166.886496	5593.968599	25.197440
167.194719	5596.559201	25.202458
166.935339	5616.077431	25.207475
167.650803	5610.321040	25.212493
167.961221	5620.633204	25.217511
167.718715	5636.673715	25.222528
167.947181	5634.936558	25.227546
168.255557	5645.889477	25.232563
168.395489	5632.260595	25.237581
168.751668	5646.871346	25.242599
168.576355	5656.824331	25.247616
169.444935	5668.208780	25.252634
169.427776	5661.883128	25.257651
169.332195	5663.931538	25.262669
169.499050	5653.690015	25.267687
169.061752	5658.064245	25.272704
169.713148	5665.947674	25.277722
169.714593	5685.432280	25.282739
169.904402	5678.456811	25.287757
170.129824	5687.473423	25.292775
170.331601	5704.091456	25.297792
170.550323	5704.853778	25.302810
170.700260	5714.112172	25.307827
170.675681	5712.892907	25.312845
171.170859	5720.628974	25.317863
171.157620	5734.134316	25.322880
171.651576	5722.861090	25.327898
171.866971	5724.985810	25.332915
172.039676	5730.431135	25.337933
172.165642	5720.786935	25.342951
172.060237	5732.807423	25.347968
172.378783	5714.865338	25.352986
172.059795	5731.415371	25.358003
172.273942	5753.840865	25.363021
172.791537	5749.710716	25.368039
172.585419	5760.920406	25.373056
172.741380	5758.601583	25.378074
172.933500	5782.493993	25.383091
173.320537	5792.096212	25.388109
173.518304	5775.525741	25.393127
173.072923	5799.489918	25.398144
173.525879	5804.940942	25.403162
173.631851	5809.639290	25.408179
173.877189	5836.352477	25.413197
174.611113	5832.138251	25.418215
174.024079	5844.908292	25.423232
174.439244	5845.033500	25.428250
174.990545	5852.437331	25.433267
175.042734	5871.126546	25.438285
175.369339	5866.758531	25.443303
175.008152	5888.327121	25.448320
175.565114	5882.248150	25.453338
175.630411	5895.804847	25.458355
175.902605	5902.697749	25.463373
176.603548	5912.879410	25.468391
176.505142	5922.880892	25.473408
176.607652	5918.100921	25.478426
176.928938	5914.433957	25.483443
177.202004	5911.418253	25.488461
177.310345	5907.621594	25.493479
177.534875	5908.191818	25.498496
177.766017	5911.018207	25.503514
177.527315	5928.631949	25.508531
177.736472	5942.676362	25.513549
178.173413	5930.689035	25.518567
178.049640	5939.850377	25.523584
178.170958	5937.256962	25.528602
178.270477	5938.238139	25.533619
178.448347	5946.915529	25.538637
178.677103	5961.950519	25.543655
178.734761	5966.219965	25.548672
179.131277	5977.441528	25.553690
179.373677	5997.578124	25.558707
179.249096	5988.325379	25.563725
179.709297	5997.558877	25.568743
179.477008	6010.359047	25.573760
180.062453	6009.017328	25.578778
180.031723	6019.569837	25.583795
180.464525	6034.729724	25.588813
180.461957	6043.112576	25.593831
180.494191	6051.540237	25.598848
180.775742	6044.270669	25.603866
180.860744	6054.976269	25.608883
180.751598	6075.109220	25.613901
181.408232	6062.872761	25.618919
181.212429	6078.071540	25.623936
181.710063	6084.601291	25.628954
182.020374	6103.718564	25.633971
182.092969	6098.859119	25.638989
182.469513	6103.537241	25.644007
182.581630	6097.708488	25.649024
182.980472	6102.968412	25.654042
183.142786	6119.270629	25.659059
183.205402	6119.712468	25.664077
183.656138	6121.217516	25.669095
183.377181	6128.621675	25.674112
183.496928	6123.506872	25.679130
183.759978	6124.642162	25.684148
183.480433	6131.710464	25.689165
184.010561	6152.841514	25.694183
184.273634	6158.853231	25.699200
184.346713	6154.488571	25.704218
184.663218	6170.368155	25.709236
184.435150	6180.442410	25.714253
184.842853	6172.285641	25.719271
184.948418	6181.295701	25.724288
185.117389	6202.244433	25.729306
185.280731	6209.628472	25.734324
185.308401	6211.472415	25.739341
185.929333	6223.907007	25.744359
185.839163	6228.783885	25.749376
186.077605	6245.118950	25.754394
186.480540	6257.694539	25.759412
186.109512	6258.535176	25.764429
186.597457	6279.774628	25.769447
186.456076	6287.373298	25.774464
186.857989	6289.226824	25.779482
187.254732	6309.962371	25.784500
187.030702	6324.957404	25.789517
187.518139	6321.196978	25.794535
187.692494	6349.948378	25.799552
187.820093	6350.125733	25.804570
188.562887	6364.501683	25.809588
188.288326	6383.640177	25.814605
188.730546	6378.436111	25.819623
188.654452	6395.122825	25.824640
189.164230	6404.161421	25.829658
189.070010	6420.080788	25.834676
189.262355	6408.076998	25.839693
189.735490	6423.543997	25.844711
189.826306	6440.178976	25.849728
189.983064	6455.094552	25.854746
190.178652	6435.724294	25.859764
190.111491	6457.284600	25.864781
190.648457	6466.871228	25.869799
190.481501	6471.481903	25.874816
190.528388	6478.577007	25.879834
191.000372	6485.975712	25.884852
191.078506	6492.369531	25.889869
191.443136	6494.273088	25.894887
191.645045	6494.786361	25.899904
191.938292	6521.383786	25.904922
192.249569	6513.300427	25.909940
192.245819	6530.839660	25.914957
192.663325	6522.595378	25.919975
192.854269	6518.859354	25.924992
192.476430	6520.172379	25.930010
192.909619	6545.857674	25.935028
193.059970	6552.074779	25.940045
193.225908	6554.313724	25.945063
193.089861	6556.275865	25.950080
193.487790	6572.788073	25.955098
194.083845	6572.649991	25.960116
194.015474	6594.813376	25.965133
194.290304	6600.227007	25.970151
194.653507	6609.215925	25.975168
194.702420	6608.334995	25.980186
194.929319	6604.132941	25.985204
195.003970	6625.628397	25.990221
195.494242	6621.298590	25.995239
195.519669	6625.316081	26.000256
195.243298	6626.310808	26.005274
195.740747	6638.112394	26.010292
196.079153	6660.129988	26.015309
196.309195	6647.487408	26.020327
196.585787	6673.559818	26.025344
196.885665	6674.170779	26.030362
197.105994	6686.066150	26.035380
196.976956	6681.084447	26.040397
197.489987	6670.515591	26.045415
197.567779	6700.755959	26.050432
197.564291	6703.168282	26.055450
197.972133	6701.000353	26.060468
198.150747	6712.275314	26.065485
198.213368	6718.857389	26.070503
198.532217	6730.010083	26.075520
198.647740	6731.315287	26.080538
198.712534	6727.240538	26.085556
198.819701	6754.709928	26.090573
199.265892	6757.044278	26.095591
199.304499	6764.415435	26.100608
199.455729	6782.815417	26.105626
199.986345	6781.214077	26.110644
199.661671	6792.777048	26.115661
199.875010	6802.996940	26.120679
200.536817	6806.389016	26.125696
200.500293	6819.574894	26.130714
200.799292	6822.758870	26.135732
200.661048	6830.492647	26.140749
201.095247	6833.822663	26.145767
201.161396	6851.019884	26.150784
201.155639	6869.144437	26.155802
202.156946	6873.708260	26.160820
201.972918	6878.385513	26.165837
201.810873	6874.305973	26.170855
201.987434	6878.880107	26.175872
202.302922	6900.048020	26.180890
202.544626	6909.032887	26.185908
202.575890	6918.938833	26.190925
203.047641	6925.530527	26.195943
203.107764	6935.902400	26.200960
203.251001	6950.460269	26.205978
203.557243	6946.363493	26.210996
204.007888	6955.477163	26.216013
203.835857	6965.296740	26.221031
204.258039	6967.209284	26.226048
204.356418	6996.952065	26.231066
204.464634	6990.922946	26.236084
204.631479	7008.996550	26.241101
204.903319	7018.973579	26.246119
205.219735	7036.293203	26.251136
205.070346	7048.630200	26.256154
205.400311	7055.241407	26.261172
205.440525	7071.228951	26.266189
205.789803	7076.812645	26.271207
206.156758	7075.255464	26.276224
206.495958	7104.705139	26.281242
206.730807	7099.537819	26.286260
206.793950	7110.246880	26.291277
207.169244	7120.610341	26.296295
207.419360	7126.685105	26.301312
207.212403	7131.719377	26.306330
208.191545	7130.655505	26.311348
208.185511	7151.656296	26.316365
208.230193	7162.102390	26.321383
208.897863	7150.538388	26.326400
209.080258	7145.059963	26.331418
209.340997	7143.636157	26.336436
208.778180	7155.079219	26.341453
209.388488	7167.824743	26.346471
209.459120	7167.188957	26.351488
209.364222	7189.025415	26.356506
209.778011	7197.543187	26.361524
210.089978	7208.118233	26.366541
210.317236	7212.006142	26.371559
210.499907	7222.070699	26.376576
210.733377	7244.782566	26.381594
211.377740	7228.040146	26.386612
211.156101	7240.580019	26.391629
211.428886	7252.830214	26.396647
211.632808	7265.071725	26.401664
211.574745	7264.240858	26.406682
211.958782	7263.833645	26.411700
212.386211	7289.753268	26.416717
212.377473	7282.934596	26.421735
212.801250	7294.748454	26.426752
212.918840	7296.623048	26.431770
213.180304	7301.479629	26.436788
213.258916	7319.444930	26.441805
213.565133	7320.331878	26.446823
214.003362	7316.391787	26.451840
213.318256	7320.355138	26.456858
213.929956	7333.478266	26.461876
213.770883	7346.970556	26.466893
214.003525	7342.709941	26.471911
214.394647	7365.952370	26.476928
214.449595	7376.808495	26.481946
214.871334	7388.037345	26.486964
215.381629	7411.182163	26.491981
215.049251	7419.630170	26.496999
215.828829	7416.568045	26.502016
215.824492	7432.543015	26.507034
216.154571	7443.932872	26.512052
216.367714	7437.304583	26.517069
216.237677	7457.131146	26.522087
216.560323	7457.688157	26.527104
216.828352	7469.796084	26.532122
217.325060	7490.213631	26.537140
217.586884	7493.310046	26.542157
217.581902	7507.806324	26.547175
218.073313	7505.562802	26.552192
217.945160	7511.484004	26.557210
218.365669	7525.821198	26.562228
218.607059	7520.595251	26.567245
218.440479	7544.225078	26.572263
218.787688	7548.086873	26.577280
218.862192	7553.868774	26.582298
218.998824	7573.553053	26.587316
219.231517	7592.555581	26.592333
219.401963	7615.024696	26.597351
219.818504	7612.055028	26.602368
220.020334	7626.260366	26.607386
220.061249	7637.510770	26.612404
220.699090	7639.312704	26.617421
221.004991	7662.801304	26.622439
221.220796	7666.884726	26.627456
221.270060	7670.396687	26.632474
221.741795	7678.342900	26.637492
222.071030	7684.897068	26.642509
222.152772	7693.219413	26.647527
222.609392	7689.695689	26.652544
222.571324	7686.800049	26.657562
222.725986	7702.498562	26.662580
223.192163	7712.734645	26.667597
223.272550	7725.566701	26.672615
223.318484	7727.987835	26.677632
223.247824	7733.957400	26.682650
223.698556	7741.817295	26.687668
224.001147	7751.916602	26.692685
223.981661	7774.884416	26.697703
224.676929	7763.368267	26.702720
224.508058	7772.042989	26.707738
224.632964	7797.225650	26.712756
224.651877	7802.527869	26.717773
224.977396	7807.357096	26.722791
225.258178	7824.722666	26.727808
225.616644	7825.062317	26.732826
225.523034	7840.019984	26.737844
225.597986	7850.039976	26.742861
225.813884	7868.726069	26.747879
226.576865	7887.225044	26.752896
226.765222	7904.671537	26.757914
226.573100	7905.600192	26.762932
227.231509	7930.307749	26.767949
227.619179	7918.326690	26.772967
227.631019	7933.119710	26.777984
227.595088	7950.309294	26.783002
227.980068	7959.594577	26.788020
228.306430	7957.021637	26.793037
228.521679	7979.153674	26.798055
228.774646	7976.058932	26.803072
228.876846	7997.592111	26.808090
229.161840	8001.221588	26.813108
229.817643	8010.254424	26.818125
229.474001	8025.890287	26.823143
230.132173	8030.107094	26.828160
230.259048	8033.900274	26.833178
230.778809	8057.529307	26.838196
230.908850	8063.892710	26.843213
230.910602	8065.730786	26.848231
231.245181	8064.223521	26.853248
231.563015	8074.582649	26.858266
231.420236	8091.595070	26.863284
231.583588	8096.598962	26.868301
231.915959	8111.946173	26.873319
231.907027	8112.782689	26.878336
231.893704	8147.284941	26.883354
232.572161	8151.481239	26.888372
232.818642	8169.276807	26.893389
232.961231	8178.730701	26.898407
233.408013	8186.486808	26.903424
233.910423	8194.680213	26.908442
233.650931	8208.038205	26.913460
234.108194	8215.879213	26.918477
234.053606	8239.234975	26.923495
234.625762	8228.931802	26.928512
234.846508	8264.851963	26.933530
234.946857	8267.096905	26.938548
235.666502	8264.163780	26.943565
235.624113	8293.590869	26.948583
235.979257	8289.183379	26.953600
236.432440	8301.991129	26.958618
236.757439	8294.147383	26.963636
236.692277	8301.599975	26.968653
236.635761	8319.280742	26.973671
236.616662	8315.877166	26.978688
236.992011	8338.567695	26.983706
237.044712	8341.793626	26.988724
237.581502	8335.980898	26.993741
237.607873	8363.138790	26.998759
238.031252	8380.594017	27.003776
238.152952	8378.732325	27.008794
238.547090	8401.202379	27.013812
238.715922	8401.600604	27.018829
239.204400	8411.289088	27.023847
238.921591	8419.439388	27.028864
239.364464	8428.239667	27.033882
239.478232	8440.852983	27.038900
239.968025	8438.730377	27.043917
239.893392	8469.124930	27.048935
240.296478	8470.679932	27.053952
240.439513	8474.558387	27.058970
240.756313	8493.887420	27.063988
240.864636	8491.423509	27.069005
241.289535	8516.415169	27.074023
241.610958	8522.602293	27.079040
241.676561	8544.347082	27.084058
241.895954	8546.729290	27.089076
242.326809	8551.650958	27.094093
242.519669	8570.905419	27.099111
243.059526	8582.582196	27.104128
243.218734	8581.608422	27.109146
243.216851	8600.006730	27.114164
243.760586	8604.583070	27.119181
243.979192	8606.935119	27.124199
244.410890	8630.237191	27.129216
244.354641	8634.002664	27.134234
244.433093	8644.875638	27.139252
244.935416	8637.303654	27.144269
244.999709	8680.682865	27.149287
245.038893	8671.238664	27.154304
245.345279	8691.629185	27.159322
245.394913	8709.330083	27.164340
245.905803	8714.568370	27.169357
246.221541	8733.070447	27.174375
246.712986	8724.799016	27.179392
247.057258	8751.644507	27.184410
247.004328	8762.659693	27.189428
247.416763	8752.537827	27.194445
247.757310	8760.471700	27.199463
247.758403	8773.132372	27.204480
247.872395	8792.786458	27.209498
248.278712	8799.306408	27.214516
248.639875	8803.021914	27.219533
248.931379	8821.413861	27.224551
249.335484	8817.783364	27.229568
249.297793	8831.494110	27.234586
249.032113	8850.498206	27.239604
249.593137	8853.476003	27.244621
249.381040	8877.249751	27.249639
249.593706	8888.616154	27.254656
250.205765	8886.722273	27.259674
250.175196	8901.920798	27.264692
250.383260	8925.174385	27.269709
250.700463	8937.789924	27.274727
251.016794	8943.132489	27.279744
251.598815	8957.289120	27.284762
251.544936	8984.475490	27.289780
252.094583	8985.059339	27.294797
252.119010	8999.206129	27.299815
251.824118	9007.202075	27.304832
252.535499	9019.387359	27.309850
252.852742	9050.370628	27.314868
253.278596	9054.328883	27.319885
253.237131	9070.073476	27.324903
253.655224	9073.512027	27.329920
253.880687	9094.972449	27.334938
254.098008	9120.173694	27.339956
254.487111	9118.419986	27.344973
254.615180	9130.263167	27.349991
254.662219	9148.219570	27.355008
255.218109	9154.100848	27.360026
255.329848	9187.003434	27.365044
255.696033	9190.508913	27.370061
256.113320	9213.601329	27.375079
256.213956	9211.751155	27.380096
256.636144	9233.561689	27.385114
256.612327	9245.897398	27.390132
257.135292	9251.327933	27.395149
257.565065	9262.878785	27.400167
257.489661	9266.184749	27.405184
258.193016	9286.894867	27.410202
257.999535	9309.458379	27.415220
258.521386	9305.534750	27.420237
258.617037	9330.889130	27.425255
258.969780	9332.669448	27.430272
259.107853	9353.923434	27.435290
258.946362	9372.226940	27.440308
259.492839	9365.381776	27.445325
259.725141	9388.775443	27.450343
260.046309	9407.700081	27.455360
260.491387	9412.040973	27.460378
260.790065	9425.746258	27.465396
261.133930	9448.356143	27.470413
261.109190	9458.405303	27.475431
261.143536	9478.403108	27.480448
261.954357	9477.544188	27.485466
261.673969	9497.918770	27.490484
262.535739	9503.379994	27.495501
262.440108	9513.994897	27.500519
262.780661	9528.121309	27.505536
263.500445	9537.489967	27.510554
263.793850	9551.827344	27.515572
263.699108	9566.007435	27.520589
264.050007	9566.918099	27.525607
264.023886	9587.654802	27.530624
264.638546	9590.519932	27.535642
264.780234	9607.534372	27.540660
264.877461	9599.806919	27.545677
265.549033	9615.924771	27.550695
265.242217	9622.292367	27.555712
265.995493	9627.606457	27.560730
266.127277	9631.382343	27.565748
266.301840	9645.258314	27.570765
266.383021	9660.616468	27.575783
266.194089	9670.131232	27.580800
266.702061	9677.459314	27.585818
266.710100	9704.160613	27.590836
267.065722	9717.578111	27.595853
267.461925	9729.689484	27.600871
267.329480	9762.918315	27.605888
267.867544	9772.558078	27.610906
268.194794	9793.352457	27.615924
268.334206	9811.366151	27.620941
269.112300	9829.458283	27.625959
269.088103	9844.822797	27.630976
269.252164	9853.738011	27.635994
269.564874	9872.005104	27.641012
269.900165	9890.448837	27.646029
270.121667	9898.305102	27.651047
270.189152	9918.451671	27.656064
270.743430	9923.192405	27.661082
271.354088	9950.592146	27.666100
271.576616	9975.320241	27.671117
271.586343	9979.814110	27.676135
271.842306	10003.010975	27.681152
272.754448	10004.717169	27.686170
272.706198	10012.310355	27.691188
272.759394	10024.634428	27.696205
273.615445	10016.764566	27.701223
273.569167	10039.792849	27.706240
273.996002	10046.053131	27.711258
274.054282	10061.727776	27.716276
274.473920	10065.385096	27.721293
274.538591	10079.974282	27.726311
274.650862	10103.503096	27.731328
275.317262	10104.200210	27.736346
275.532187	10124.491183	27.741364
275.809673	10123.686944	27.746381
276.240669	10129.795891	27.751399
276.443640	10146.094856	27.756416
276.785133	10147.799159	27.761434
277.030106	10155.729730	27.766452
277.374201	10169.460331	27.771469
277.203725	10180.464992	27.776487
277.482680	10186.039042	27.781504
278.200936	10190.477889	27.786522
278.358720	10204.009991	27.791540
278.465083	10207.018040	27.796557
278.941053	10222.376410	27.801575
278.882844	10222.948206	27.806592
279.267917	10253.205811	27.811610
278.906151	10265.403408	27.816628
279.318437	10276.539154	27.821645
279.672340	10291.385832	27.826663
279.766137	10308.523994	27.831680
280.365208	10331.435698	27.836698
280.586532	10332.220292	27.841716
280.668390	10356.392994	27.846733
281.066597	10365.531295	27.851751
280.744511	10383.926160	27.856768
281.313478	10408.242061	27.861786
281.365178	10421.609470	27.866804
281.876324	10440.186792	27.871821
282.402342	10460.800493	27.876839
282.472946	10475.005060	27.881856
283.293596	10496.303762	27.886874
283.148110	10518.565521	27.891892
283.674301	10531.554799	27.896909
283.909976	10543.767971	27.901927
284.406313	10562.688972	27.906944
284.477268	10573.907282	27.911962
284.753139	10607.514799	27.916980
285.239122	10600.368647	27.921997
285.915027	10626.050630	27.927015
285.622027	10643.348411	27.932032
286.265993	10644.958130	27.937050
286.667748	10664.715188	27.942068
286.638752	10668.923453	27.947085
287.420968	10680.939447	27.952103
287.503702	10693.965704	27.957120
287.624886	10704.009357	27.962138
287.888538	10724.205424	27.967156
288.173194	10734.687777	27.972173
288.371548	10742.042911	27.977191
288.205244	10774.957084	27.982208
288.703550	10788.465346	27.987226
288.996469	10806.083900	27.992244
289.234229	10826.206119	27.997261
289.544611	10838.249432	28.002279
289.787674	10860.166833	28.007296
290.411576	10855.355710	28.012314
290.671055	10884.339953	28.017332
290.922407	10887.560350	28.022349
291.530056	10900.012415	28.027367
291.738886	10906.244058	28.032384
291.846396	10928.413367	28.037402
292.219447	10941.326276	28.042420
292.651619	10958.019308	28.047437
292.984819	10969.896570	28.052455
293.146869	10974.535670	28.057472
293.246718	11000.944845	28.062490
293.105400	11018.103972	28.067508
293.777706	11024.736769	28.072525
294.219428	11050.306874	28.077543
294.259421	11076.507713	28.082560
294.667769	11081.401548	28.087578
295.224508	11096.085260	28.092596
295.333214	11104.164372	28.097613
295.783130	11118.556613	28.102631
295.726173	11130.731508	28.107648
296.110860	11139.544245	28.112666
296.261298	11164.238954	28.117684
296.520723	11174.897997	28.122701
297.241752	11186.352762	28.127719
297.361711	11210.551848	28.132736
297.719520	11213.415348	28.137754
297.991161	11230.138203	28.142772
297.958320	11234.026126	28.147789
298.433871	11256.272630	28.152807
298.590024	11272.314257	28.157824
298.848931	11294.820441	28.162842
299.333734	11304.281977	28.167860
299.301322	11334.545331	28.172877
299.890264	11333.634728	28.177895
300.306992	11350.427858	28.182912
300.340944	11362.444420	28.187930
300.914684	11379.662357	28.192948
301.226124	11404.886670	28.197965
301.383699	11411.408062	28.202983
301.721584	11429.734428	28.208000
302.163802	11443.541068	28.213018
302.565367	11450.149913	28.218036
302.353042	11471.690586	28.223053
302.995561	11495.271649	28.228071
302.991857	11510.293010	28.233088
303.410140	11528.430382	28.238106
303.865934	11546.245401	28.243124
303.929787	11568.241189	28.248141
304.502855	11561.930342	28.253159
305.054424	11598.025930	28.258176
304.943767	11604.337115	28.263194
305.690798	11619.464627	28.268212
305.798330	11644.077824	28.273229
306.348776	11653.628880	28.278247
306.359519	11670.101016	28.283264
306.856369	11674.866819	28.288282
307.091238	11689.594146	28.293300
307.324282	11705.858918	28.298317
307.668135	11720.081319	28.303335
308.078890	11739.821039	28.308352
308.160097	11749.039830	28.313370
308.648144	11769.611008	28.318388
309.013507	11785.645811	28.323405
309.318935	11788.069142	28.328423
309.356245	11809.745239	28.333440
309.973320	11811.735012	28.338458
310.326743	11827.440013	28.343476
310.600540	11856.908481	28.348493
310.752278	11857.548802	28.353511
311.166797	11865.457194	28.358528
311.480938	11871.885555	28.363546
311.910906	11892.017524	28.368564
311.727789	11913.509108	28.373581
311.993625	11903.445506	28.378599
312.088405	11932.646908	28.383616
312.300748	11959.405229	28.388634
312.804519	11962.318616	28.393652
313.024351	11985.103992	28.398669
313.141241	11996.776479	28.403687
313.655066	12029.918511	28.408704
314.104438	12037.861777	28.413722
314.579962	12070.069240	28.418740
314.803355	12087.464444	28.423757
314.940084	12088.739395	28.428775
315.733426	12108.730114	28.433792
315.715059	12129.996025	28.438810
316.209285	12137.563642	28.443828
316.177147	12153.894574	28.448845
316.818934	12186.063587	28.453863
316.986432	12187.408613	28.458880
317.259709	12205.401079	28.463898
317.730879	12218.423022	28.468916
317.766596	12243.747380	28.473933
318.133568	12264.756082	28.478951
318.688437	12272.600999	28.483968
318.663290	12296.767096	28.488986
319.218186	12314.402333	28.494004
319.266377	12336.799217	28.499021
319.852497	12351.360427	28.504039
320.443373	12367.319177	28.509056
320.728064	12382.773998	28.514074
321.159760	12406.479423	28.519092
321.056605	12424.746429	28.524109
321.540878	12440.053011	28.529127
322.119232	12447.966100	28.534144
322.110857	12474.980306	28.539162
322.418702	12486.074323	28.544180
322.615334	12509.635352	28.549197
323.126442	12530.980768	28.554215
323.303067	12559.054606	28.559232
323.474818	12566.255482	28.564250
324.238894	12592.580271	28.569268
324.092097	12611.850153	28.574285
324.717631	12622.016404	28.579303
325.241953	12646.698616	28.584320
325.015817	12681.739666	28.589338
326.099691	12689.208870	28.594356
326.005349	12707.634398	28.599373
326.677729	12723.015779	28.604391
326.950093	12738.737794	28.609408
327.577098	12745.469496	28.614426
327.956552	12754.982192	28.619444
327.931329	12771.891022	28.624461
328.127763	12787.164328	28.629479
328.739641	12803.307331	28.634496
328.807150	12816.100524	28.639514
329.423606	12821.626692	28.644532
329.435339	12835.374912	28.649549
330.043641	12838.515234	28.654567
330.124438	12849.607526	28.659584
329.887689	12860.168942	28.664602
330.656701	12864.329355	28.669620
330.941536	12895.573053	28.674637
330.936079	12913.250865	28.679655
331.466719	12930.858023	28.684672
331.467758	12939.922262	28.689690
331.843709	12962.132645	28.694708
332.251882	12990.818583	28.699725
332.467975	13004.576303	28.704743
332.848000	13029.221132	28.709760
333.043925	13063.709743	28.714778
333.692655	13075.659208	28.719796
333.688232	13105.287590	28.724813
334.073780	13137.544131	28.729831
334.506702	13144.716060	28.734848
334.650589	13173.267352	28.739866
334.967186	13192.036898	28.744884
335.381406	13231.235998	28.749901
335.786141	13244.259772	28.754919
336.346923	13261.691898	28.759936
337.012361	13292.588449	28.764954
337.785353	13301.843563	28.769972
337.888200	13328.685014	28.774989
338.261468	13342.703335	28.780007
338.606372	13334.572029	28.785024
338.873470	13364.456468	28.790042
339.113952	13367.084737	28.795060
339.641988	13382.542829	28.800077
339.642367	13393.836954	28.805095
340.110305	13418.026418	28.810112
340.135994	13438.896216	28.815130
340.724132	13449.315367	28.820148
341.022331	13471.406644	28.825165
341.159290	13496.952412	28.830183
341.894199	13507.418173	28.835200
342.163142	13521.001062	28.840218
342.657536	13546.900457	28.845236
342.646966	13560.038210	28.850253
343.018361	13583.057954	28.855271
343.468285	13591.550707	28.860288
343.739825	13613.492573	28.865306
344.024374	13641.531038	28.870324
344.233198	13662.647564	28.875341
344.505710	13686.805428	28.880359
344.900800	13702.197361	28.885376
345.053418	13734.745166	28.890394
345.336503	13753.946015	28.895412
345.785355	13775.134356	28.900429
346.369282	13803.033704	28.905447
346.712277	13816.260077	28.910464
346.922691	13843.577277	28.915482
347.393456	13842.633331	28.920500
347.666981	13866.495242	28.925517
348.003862	13887.761310	28.930535
348.426893	13895.244731	28.935552
348.662180	13909.458153	28.940570
348.834090	13928.758019	28.945588
349.244000	13949.980951	28.950605
349.692021	13977.365616	28.955623
350.382251	13995.384875	28.960640
350.496857	14021.633709	28.965658
350.574278	14029.259157	28.970676
351.516062	14034.821607	28.975693
351.866928	14065.637024	28.980711
352.333976	14065.435485	28.985728
352.347460	14077.767017	28.990746
353.100106	14103.240484	28.995764
353.376962	14111.015246	29.000781
353.722488	14126.579342	29.005799
353.641942	14136.363402	29.010816
354.025162	14156.265048	29.015834
354.458315	14168.105284	29.020852
354.929735	14195.703878	29.025869
354.865047	14222.016166	29.030887
355.317836	14233.603979	29.035904
355.705912	14249.842248	29.040922
355.876419	14267.596809	29.045940
356.640976	14292.261718	29.050957
356.880820	14318.028625	29.055975
357.087104	14338.110732	29.060992
357.066532	14367.631270	29.066010
357.596623	14371.485884	29.071028
358.096573	14402.578639	29.076045
358.504079	14432.405477	29.081063
359.346707	14444.498316	29.086080
359.675787	14471.487276	29.091098
359.748716	14487.155400	29.096116
360.222625	14507.327531	29.101133
360.565111	14528.756652	29.106151
360.988540	14535.698529	29.111168
361.088743	14570.267103	29.116186
361.286232	14579.105683	29.121204
361.977449	14605.555594	29.126221
361.921370	14631.111091	29.131239
362.358199	14637.421401	29.136256
362.731451	14679.840633	29.141274
363.224517	14680.836241	29.146292
364.231111	14703.871985	29.151309
364.834718	14702.083294	29.156327
365.449802	14730.842665	29.161344
365.565091	14738.872871	29.166362
366.124432	14734.104706	29.171380
366.643291	14748.889037	29.176397
366.432500	14753.206022	29.181415
367.075701	14750.437025	29.186432
367.289422	14760.507096	29.191450
367.473040	14778.085496	29.196468
367.628142	14790.936942	29.201485
367.600042	14810.968161	29.206503
368.012336	14813.922772	29.211520
368.160113	14834.186764	29.216538
368.423131	14858.060854	29.221556
368.747575	14884.735210	29.226573
368.770855	14894.519151	29.231591
369.488694	14923.713299	29.236608
369.772635	14950.304971	29.241626
370.084408	14971.600956	29.246644
370.445659	15001.512761	29.251661
370.711902	15032.798240	29.256679
371.087262	15052.396761	29.261696
371.463622	15075.397598	29.266714
371.616534	15113.698977	29.271732
372.358769	15128.078965	29.276749
372.627473	15174.081252	29.281767
373.045391	15195.578997	29.286784
373.455061	15222.201981	29.291802
373.904996	15246.818493	29.296820
374.496835	15280.135949	29.301837
374.491299	15300.393891	29.306855
375.524047	15317.124749	29.311872
375.813679	15349.866713	29.316890
376.009676	15376.978850	29.321908
376.561537	15382.384202	29.326925
376.758718	15412.621716	29.331943
377.223676	15424.327276	29.336960
377.363283	15459.446197	29.341978
377.757886	15469.585139	29.346996
378.509922	15497.441317	29.352013
378.796101	15524.360931	29.357031
379.605135	15538.387614	29.362048
379.517668	15558.636021	29.367066
379.590027	15592.397302	29.372084
380.096610	15601.280906	29.377101
380.508355	15646.920045	29.382119
381.022555	15652.873333	29.387136
381.472347	15683.893432	29.392154
381.790097	15717.075522	29.397172
382.240572	15723.709552	29.402189
382.357960	15756.854965	29.407207
382.950526	15775.609500	29.412224
383.515572	15804.105875	29.417242
383.573194	15833.157688	29.422260
384.296442	15837.075690	29.427277
384.481049	15870.403126	29.432295
384.690304	15882.368351	29.437312
385.425453	15921.121306	29.442330
385.815179	15931.312407	29.447348
386.524480	15944.089011	29.452365
386.470376	15972.784536	29.457383
386.895589	15983.299693	29.462400
387.344064	16010.202270	29.467418
387.223562	16021.490922	29.472436
387.665351	16052.378119	29.477453
388.211043	16077.040836	29.482471
388.463160	16086.765256	29.487488
388.581123	16110.444556	29.492506
388.976433	16125.710966	29.497524
389.692394	16150.550974	29.502541
389.915795	16193.954043	29.507559
390.440939	16204.280027	29.512576
390.859225	16228.999701	29.517594
390.900718	16255.448922	29.522612
391.643534	16277.723770	29.527629
391.862005	16304.017529	29.532647
391.983075	16334.056704	29.537664
392.679817	16354.850607	29.542682
393.073089	16389.206811	29.547700
393.346322	16403.831218	29.552717
393.826457	16440.577149	29.557735
394.153814	16462.940509	29.562752
394.973716	16477.858744	29.567770
394.903094	16516.826816	29.572788
395.770100	16525.538879	29.577805
396.195705	16549.030086	29.582823
396.261148	16569.930578	29.587840
397.243631	16595.471869	29.592858
397.390306	16613.771959	29.597876
397.782200	16636.714793	29.602893
397.771204	16660.331242	29.607911
398.506045	16688.603208	29.612928
398.933472	16716.723835	29.617946
398.753626	16750.296657	29.622964
399.535351	16773.929084	29.627981
399.698746	16776.734489	29.632999
400.277490	16822.703128	29.638016
400.718094	16848.079432	29.643034
401.014697	16874.038120	29.648052
401.780414	16893.669702	29.653069
401.896122	16929.392085	29.658087
402.441917	16941.697982	29.663104
403.167642	16975.216761	29.668122
403.067556	16999.811622	29.673140
403.881905	17014.624189	29.678157
404.233199	17040.101056	29.683175
404.611884	17053.584367	29.688192
404.915908	17079.377468	29.693210
405.251442	17110.295920	29.698228
405.650846	17132.963316	29.703245
405.836513	17159.819625	29.708263
406.161703	17186.744492	29.713280
406.853225	17204.499447	29.718298
407.085832	17238.921722	29.723316
407.791986	17270.170000	29.728333
407.965891	17297.639998	29.733351
408.533207	17317.950741	29.738368
408.877227	17340.943980	29.743386
409.141660	17373.872202	29.748404
409.670433	17388.656621	29.753421
409.972904	17404.526659	29.758439
410.238467	17425.912142	29.763456
410.967707	17444.338100	29.768474
411.255312	17471.672187	29.773492
411.612964	17493.695026	29.778509
411.889613	17526.566905	29.783527
412.244592	17544.036126	29.788544
412.792953	17566.045612	29.793562
413.162076	17578.071915	29.798580
413.527761	17610.062500	29.803597
414.028927	17635.964484	29.808615
414.289880	17670.493827	29.813632
415.155982	17685.692485	29.818650
415.358139	17717.094801	29.823668
415.773125	17733.416133	29.828685
415.808238	17768.319854	29.833703
415.982006	17792.327474	29.838720
416.595592	17821.277907	29.843738
416.976946	17865.200051	29.848756
417.713813	17888.114584	29.853773
418.065024	17919.924655	29.858791
418.554721	17938.638578	29.863808
419.392291	17970.061426	29.868826
419.469983	17997.014538	29.873844
419.816332	18014.066774	29.878861
420.550046	18043.011475	29.883879
420.911453	18080.288287	29.888896
421.691054	18097.509380	29.893914
422.089356	18118.236488	29.898932
422.411561	18139.911567	29.903949
422.476084	18154.851397	29.908967
422.674047	18184.021089	29.913984
423.363162	18204.329539	29.919002
423.750386	18244.309710	29.924020
424.081272	18268.822955	29.929037
424.574443	18288.458009	29.934055
424.668481	18322.621302	29.939072
425.409100	18348.524910	29.944090
425.607036	18388.809628	29.949108
426.275877	18416.497636	29.954125
426.836991	18440.180762	29.959143
426.954599	18474.293781	29.964160
427.394959	18480.510146	29.969178
428.077261	18517.329001	29.974196
428.422204	18540.234897	29.979213
429.141383	18581.441416	29.984231
429.179435	18604.523863	29.989248
430.160556	18623.907976	29.994266
430.401957	18640.157918	29.999284
430.809483	18659.248807	30.004301
431.418404	18694.147440	30.009319
431.464352	18713.873972	30.014336
431.962621	18736.897072	30.019354
432.336331	18758.042746	30.024372
432.687613	18781.201144	30.029389
432.952169	18806.645128	30.034407
433.233600	18828.655630	30.039424
433.886146	18852.811452	30.044442
434.050772	18884.560309	30.049460
434.914537	18914.570215	30.054477
435.365489	18936.750721	30.059495
435.273502	18968.717412	30.064512
435.921781	19001.813533	30.069530
436.448465	19027.309428	30.074548
436.580443	19042.125577	30.079565
437.315960	19072.175513	30.084583
437.539530	19111.773729	30.089600
438.038489	19142.396558	30.094618
438.306191	19168.009932	30.099636
438.879691	19192.683237	30.104653
439.314247	19220.053292	30.109671
439.598774	19253.382321	30.114688
440.286850	19284.012703	30.119706
440.439663	19320.147689	30.124724
440.912104	19346.693371	30.129741
441.509056	19378.895259	30.134759
441.917997	19414.343154	30.139776
442.488037	19436.907399	30.144794
442.724517	19472.947118	30.149812
443.355272	19510.516360	30.154829
444.076458	19532.825937	30.159847
444.234284	19573.670545	30.164864
445.024625	19590.822298	30.169882
445.253088	19616.880887	30.174900
445.717215	19657.280817	30.179917
446.246474	19675.248736	30.184935
446.390752	19720.637639	30.189952
447.220181	19744.997399	30.194970
447.333436	19769.751636	30.199988
447.577194	19800.928277	30.205005
448.465379	19830.975045	30.210023
448.644199	19863.387083	30.215040
449.175480	19893.068740	30.220058
449.474657	19936.212097	30.225076
449.912756	19960.729432	30.230093
450.639484	19998.065637	30.235111
450.862556	20038.457313	30.240128
451.364674	20066.834348	30.245146
451.954097	20099.451177	30.250164
452.097977	20138.075988	30.255181
452.966498	20156.146339	30.260199
452.990112	20201.118795	30.265216
453.168840	20229.992584	30.270234
453.967678	20267.562464	30.275252
454.863344	20298.640965	30.280269
455.467279	20333.893324	30.285287
455.381847	20362.059734	30.290304
456.231515	20385.361225	30.295322
456.726129	20415.300931	30.300340
457.064753	20435.604747	30.305357
457.773705	20450.739820	30.310375
458.007938	20477.930578	30.315392
458.258634	20501.089442	30.320410
458.917775	20527.747962	30.325428
459.085908	20562.848973	30.330445
459.580745	20585.086653	30.335463
459.979391	20611.626949	30.340480
460.225717	20637.721799	30.345498
460.676885	20684.313216	30.350516
460.933036	20720.123896	30.355533
461.749337	20738.689147	30.360551
462.045439	20779.162056	30.365568
462.755052	20810.557484	30.370586
463.098926	20849.989725	30.375604
463.179367	20878.976445	30.380621
463.818876	20909.590981	30.385639
464.654720	20953.923906	30.390656
465.262525	20982.154246	30.395674
465.600561	21002.152932	30.400692
465.905975	21037.141384	30.405709
466.396737	21069.284132	30.410727
466.652882	21116.192990	30.415744
467.042510	21139.210169	30.420762
467.636820	21186.676501	30.425780
467.939646	21223.132982	30.430797
468.822038	21249.873331	30.435815
469.159112	21297.175425	30.440832
469.900897	21319.249193	30.445850
470.121987	21362.699913	30.450868
470.898081	21391.842164	30.455885
471.746573	21414.623623	30.460903
472.001464	21443.769456	30.465920
472.494366	21471.476352	30.470938
473.085908	21497.344372	30.475956
473.408734	21523.200113	30.480973
474.280432	21552.669236	30.485991
474.311623	21591.094657	30.491008
474.676279	21613.851099	30.496026
474.846812	21641.660055	30.501044
475.671012	21682.836371	30.506061
475.759223	21716.055815	30.511079
476.102675	21752.494449	30.516096
476.512618	21787.830992	30.521114
477.147841	21822.581995	30.526132
477.685336	21855.334007	30.531149
478.235539	21902.047932	30.536167
478.873118	21928.322023	30.541184
479.218964	21963.606163	30.546202
480.184231	21996.524238	30.551220
480.274255	22025.773020	30.556237
481.000260	22050.941629	30.561255
481.330437	22091.525109	30.566272
481.848231	22111.097261	30.571290
482.345130	22152.490765	30.576308
482.729929	22170.598769	30.581325
483.365590	22198.581129	30.586343
483.669051	22240.287639	30.591360
483.893138	22259.555493	30.596378
484.535339	22297.322163	30.601396
484.735169	22323.819442	30.606413
485.302768	22347.915050	30.611431
485.791199	22384.937721	30.616448
486.105393	22431.304882	30.621466
486.918853	22459.340507	30.626484
487.003447	22486.983490	30.631501
487.947944	22525.626422	30.636519
488.199022	22559.370663	30.641536
488.673729	22581.527347	30.646554
489.322343	22614.536541	30.651572
489.365187	22658.690274	30.656589
490.345325	22677.805909	30.661607
490.754017	22724.952014	30.666624
491.215587	22759.646895	30.671642
491.730666	22792.006673	30.676660
492.194387	22827.138494	30.681677
492.686135	22865.328243	30.686695
493.274655	22908.221388	30.691712
493.573376	22943.612891	30.696730
494.443425	22967.181597	30.701748
494.632816	23016.902061	30.706765
495.372205	23040.371968	30.711783
495.700205	23080.622799	30.716800
495.750322	23118.682660	30.721818
496.797451	23156.943748	30.726836
497.216668	23180.794103	30.731853
497.768816	23221.003283	30.736871
498.013236	23252.563544	30.741888
498.567772	23301.464288	30.746906
499.163746	23323.263218	30.751924
499.375898	23375.421335	30.756941
499.861987	23409.926273	30.761959
500.800756	23450.013012	30.766976
501.001639	23484.799055	30.771994
501.860572	23517.904234	30.777012
502.185776	23561.188452	30.782029
502.704254	23595.850107	30.787047
503.334697	23626.971542	30.792064
503.701050	23679.277018	30.797082
504.572260	23699.959815	30.802100
504.784018	23736.735129	30.807117
505.086218	23770.591168	30.812135
505.612776	23810.254544	30.817152
505.966171	23858.826713	30.822170
506.824180	23883.540058	30.827188
507.264696	23923.155983	30.832205
507.539618	23966.361880	30.837223
508.207733	24011.806103	30.842240
508.358976	24040.617195	30.847258
509.393115	24071.647628	30.852276
509.534966	24111.000457	30.857293
510.245698	24150.952001	30.862311
510.914193	24177.385601	30.867328
511.304095	24212.503893	30.872346
511.483547	24236.723286	30.877364
511.900497	24275.158352	30.882381
512.359701	24301.253701	30.887399
512.868095	24345.106376	30.892416
513.283885	24391.457565	30.897434
514.086541	24413.980488	30.902452
514.362749	24471.257616	30.907469
515.138717	24508.386748	30.912487
515.611647	24540.774138	30.917504
516.020469	24578.009964	30.922522
516.231755	24619.223815	30.927540
516.627832	24661.008582	30.932557
517.516591	24704.457424	30.937575
518.251020	24743.028165	30.942592
518.704827	24793.334363	30.947610
519.639036	24831.930214	30.952628
519.978499	24863.527370	30.957645
520.290075	24901.692422	30.962663
520.933498	24939.124104	30.967680
521.414102	24985.759734	30.972698
521.958446	25018.269847	30.977716
522.658269	25072.397660	30.982733
523.036702	25091.723928	30.987751
523.800547	25126.382134	30.992768
524.010220	25183.598366	30.997786
525.032934	25206.292178	31.002804
525.112886	25263.164629	31.007821
525.326112	25305.156662	31.012839
526.100496	25331.253913	31.017856
526.849677	25373.391569	31.022874
527.314502	25423.050459	31.027892
527.647396	25453.557994	31.032909
528.035679	25509.668498	31.037927
528.717862	25548.733984	31.042944
529.043855	25595.856863	31.047962
529.945185	25616.702011	31.052980
530.706937	25673.056105	31.057997
530.762983	25714.470025	31.063015
531.681473	25738.869397	31.068032
531.972216	25795.110664	31.073050
532.793729	25839.699045	31.078068
533.194647	25880.384124	31.083085
533.585388	25903.262309	31.088103
534.273118	25946.275460	31.093120
534.463232	25995.006965	31.098138
535.036860	26026.306787	31.103156
535.815061	26063.940219	31.108173
536.240252	26108.476669	31.113191
536.881530	26149.283280	31.118208
537.284438	26186.972838	31.123226
537.889454	26219.964165	31.128244
538.408378	26262.793924	31.133261
538.903896	26290.628568	31.138279
539.514808	26331.928918	31.143296
539.753254	26375.132952	31.148314
540.471200	26410.570941	31.153332
540.911684	26444.266450	31.158349
541.195321	26479.309746	31.163367
542.028897	26519.252379	31.168384
542.302093	26567.657261	31.173402
543.264784	26595.365242	31.178420
543.618499	26647.315318	31.183437
543.994065	26687.082368	31.188455
544.922642	26716.036021	31.193472
545.023588	26763.279315	31.198490
545.792772	26793.746697	31.203508
546.712292	26829.057390	31.208525
547.082235	26883.512512	31.213543
547.797651	26913.000745	31.218560
548.372386	26961.179946	31.223578
548.824893	26987.778660	31.228596
549.430543	27038.356854	31.233613
549.782391	27072.238758	31.238631
550.460759	27112.343097	31.243648
550.631245	27153.930000	31.248666
551.087966	27195.082226	31.253684
551.846400	27235.737430	31.258701
552.212949	27287.975092	31.263719
553.063849	27327.627836	31.268736
553.686261	27365.148897	31.273754
554.075675	27407.368109	31.278772
554.314251	27457.805180	31.283789
554.972289	27499.209747	31.288807
556.121219	27556.296644	31.293824
555.985335	27604.204894	31.298842
557.060103	27630.889136	31.303860
557.594573	27688.444662	31.308877
557.960695	27726.584103	31.313895
558.710816	27767.590213	31.318912
559.184276	27815.430402	31.323930
560.012460	27848.952074	31.328948
560.654874	27896.841231	31.333965
560.952194	27935.843034	31.338983
561.946409	27964.009272	31.344000
562.069669	28013.168010	31.349018
562.822382	28050.283848	31.354036
563.369544	28087.416752	31.359053
563.618891	28140.028808	31.364071
564.284230	28175.368760	31.369088
564.558154	28215.364557	31.374106
565.248725	28262.952456	31.379124
566.088043	28321.520619	31.384141
566.418154	28362.558889	31.389159
567.216746	28402.830871	31.394176
567.412343	28454.417202	31.399194
568.156130	28475.563000	31.404212
568.852807	28510.236851	31.409229
568.740498	28558.107919	31.414247
569.695323	28591.885159	31.419264
569.926637	28638.603386	31.424282
570.864836	28674.194076	31.429300
571.149068	28718.291371	31.434317
571.559414	28776.891679	31.439335
572.433238	28820.173613	31.444352
572.853743	28873.235119	31.449370
573.337222	28907.209426	31.454388
574.175549	28959.976173	31.459405
574.583825	29003.261827	31.464423
575.386623	29047.088322	31.469440
575.644843	29088.757620	31.474458
576.323894	29135.428030	31.479476
576.924126	29182.111127	31.484493
577.328416	29236.375649	31.489511
578.328935	29278.576481	31.494528
578.702999	29338.018238	31.499546
578.977480	29380.914895	31.504564
580.029262	29416.868923	31.509581
580.850423	29471.091476	31.514599
581.534968	29524.253312	31.519616
582.104328	29577.124785	31.524634
582.559162	29601.616482	31.529652
583.143381	29633.210802	31.534669
583.745161	29678.831328	31.539687
584.487121	29717.664164	31.544704
584.712574	29774.538767	31.549722
585.254037	29820.452966	31.554740
586.075047	29868.800168	31.559757
586.340873	29913.756221	31.564775
586.928786	29960.711428	31.569792
587.540980	30013.973062	31.574810
588.155458	30050.236109	31.579828
588.508878	30122.536037	31.584845
589.122197	30171.642162	31.589863
590.247661	30208.126771	31.594880
590.887745	30262.248414	31.599898
591.015148	30300.258557	31.604916
592.184177	30352.022105	31.609933
592.781050	30395.292454	31.614951
593.361429	30442.628488	31.619968
593.558970	30488.878292	31.624986
594.030895	30524.476379	31.630004
594.759322	30586.368959	31.635021
595.239454	30635.395249	31.640039
596.340177	30681.129820	31.645056
596.412892	30725.671268	31.650074
597.190371	30774.828714	31.655092
597.929258	30812.282463	31.660109
598.006888	30866.617034	31.665127
598.680839	30921.201975	31.670144
599.442341	30969.962235	31.675162
599.722010	31009.997074	31.680180
600.584646	31059.447570	31.685197
601.196638	31106.963315	31.690215
601.825843	31156.723939	31.695232
602.368085	31207.729481	31.700250
602.944764	31239.808819	31.705268
603.876596	31285.420676	31.710285
604.089366	31336.945609	31.715303
604.656690	31390.598712	31.720320
605.001709	31432.608481	31.725338
605.492623	31482.598586	31.730356
606.653664	31522.043552	31.735373
606.870114	31575.387477	31.740391
607.753053	31628.631743	31.745408
608.463899	31670.494025	31.750426
609.037158	31721.343340	31.755444
609.762706	31764.336757	31.760461
610.234749	31830.636026	31.765479
610.741807	31879.593973	31.770496
611.391765	31925.075970	31.775514
611.994717	31970.362255	31.780532
612.919734	32014.088995	31.785549
613.176274	32081.826372	31.790567
613.888240	32128.197470	31.795584
614.530722	32162.865659	31.800602
615.155478	32217.007232	31.805620
615.702384	32279.508837	31.810637
616.016222	32328.172619	31.815655
616.807768	32383.295361	31.820672
617.486743	32447.666426	31.825690
617.714221	32500.343282	31.830708
618.855771	32551.017974	31.835725
619.155609	32615.981253	31.840743
619.653574	32671.384989	31.845760
620.530933	32719.674893	31.850778
621.116366	32771.868457	31.855796
622.353093	32826.165201	31.860813
622.487881	32888.756807	31.865831
623.017975	32945.994245	31.870848
624.003131	33009.563724	31.875866
624.585355	33066.645111	31.880884
625.308804	33110.495134	31.885901
625.676127	33164.368711	31.890919
626.466650	33213.747327	31.895936
626.967946	33262.918368	31.900954
627.400591	33321.279167	31.905972
628.179103	33365.474187	31.910989
628.655444	33419.213011	31.916007
629.377825	33468.414085	31.921024
630.298810	33531.992641	31.926042
630.689600	33578.660135	31.931060
631.271261	33628.022806	31.936077
632.083391	33689.056219	31.941095
632.643645	33740.071460	31.946112
633.252297	33786.733222	31.951130
633.579959	33842.850549	31.956148
634.313309	33893.949043	31.961165
634.683118	33941.634483	31.966183
635.664030	33992.069628	31.971200
636.055290	34050.368649	31.976218
636.734315	34104.974366	31.981236
637.343692	34149.335554	31.986253
637.626287	34209.708010	31.991271
638.481813	34260.479212	31.996288
639.581943	34315.078467	32.001306
639.711310	34373.601607	32.006324
640.236400	34420.060916	32.011341
640.797238	34480.103146	32.016359
642.018691	34528.277333	32.021376
642.621662	34584.848316	32.026394
642.952406	34638.800289	32.031412
644.118501	34690.819160	32.036429
644.723453	34748.099767	32.041447
645.127889	34801.261782	32.046464
646.250606	34842.667691	32.051482
646.821088	34911.544231	32.056500
647.806636	34956.331641	32.061517
648.359312	34996.767761	32.066535
648.820989	35048.211013	32.071552
649.660096	35094.414114	32.076570
650.117077	35145.590418	32.081588
650.960504	35188.955477	32.086605
651.436737	35249.155833	32.091623
652.039044	35296.948441	32.096640
652.810506	35344.668535	32.101658
653.187825	35404.467436	32.106676
653.848365	35463.819450	32.111693
654.536335	35512.412502	32.116711
655.048577	35561.188172	32.121728
655.582811	35622.225637	32.126746
656.296289	35687.617468	32.131764
657.061616	35744.672593	32.136781
657.845857	35792.786061	32.141799
658.422945	35848.041179	32.146816
659.002060	35901.461081	32.151834
659.467923	35957.713293	32.156852
660.306755	36024.150638	32.161869
660.653264	36093.712518	32.166887
661.206235	36157.195746	32.171904
662.186171	36204.498848	32.176922
662.496422	36276.033219	32.181940
663.670765	36329.383360	32.186957
664.252851	36394.354282	32.191975
664.783319	36447.608673	32.196992
665.642458	36504.277803	32.202010
666.012152	36571.998103	32.207028
666.883652	36632.124731	32.212045
667.440115	36685.434072	32.217063
667.955474	36750.513169	32.222080
669.162781	36810.667376	32.227098
669.797800	36868.164879	32.232116
670.325649	36919.264374	32.237133
670.961279	36970.916024	32.242151
671.446602	37017.464565	32.247168
672.104767	37064.550150	32.252186
672.557097	37120.439482	32.257204
673.518080	37176.883399	32.262221
674.138541	37223.207606	32.267239
674.570565	37285.235460	32.272256
675.669385	37339.838519	32.277274
675.884533	37402.752732	32.282292
676.742976	37463.057848	32.287309
677.322339	37515.002352	32.292327
677.789204	37587.092849	32.297344
678.363660	37634.160246	32.302362
679.172757	37706.422230	32.307380
679.883756	37772.084307	32.312397
680.391996	37829.551672	32.317415
681.456062	37895.000343	32.322432
682.445608	37953.859419	32.327450
683.157751	38017.817840	32.332468
683.979925	38060.457391	32.337485
684.750005	38126.590767	32.342503
685.098972	38182.682978	32.347520
685.993484	38236.488958	32.352538
686.465503	38294.662171	32.357556
687.555007	38331.504713	32.362573
688.461234	38394.692588	32.367591
689.012752	38461.804976	32.372608
690.110355	38493.801189	32.377626
690.390640	38561.568942	32.382644
690.859790	38611.793611	32.387661
691.593584	38672.594354	32.392679
692.185443	38727.892844	32.397696
692.837326	38783.431091	32.402714
693.495572	38856.444183	32.407732
694.121822	38905.239781	32.412749
694.813927	38968.856516	32.417767
695.174809	39022.961253	32.422784
696.193629	39088.152117	32.427802
696.606754	39154.292728	32.432820
697.471204	39215.572896	32.437837
698.359263	39284.219677	32.442855
698.866682	39341.816878	32.447872
700.176595	39396.065003	32.452890
701.149052	39457.628452	32.457908
701.688105	39516.604113	32.462925
702.380224	39571.638670	32.467943
702.786044	39621.770762	32.472960
703.943370	39670.670082	32.477978
704.457253	39723.437576	32.482996
704.750858	39776.008501	32.488013
705.614594	39832.293858	32.493031
705.817529	39900.247991	32.498048
706.633508	39959.895435	32.503066
707.159287	40023.000143	32.508084
707.978972	40083.207231	32.513101
708.787935	40131.324421	32.518119
709.345084	40206.065632	32.523136
709.863750	40245.461656	32.528154
710.395474	40311.903270	32.533172
710.758707	40381.003883	32.538189
711.917733	40438.532595	32.543207
712.313531	40518.686138	32.548224
713.232085	40579.495828	32.553242
713.871454	40643.075181	32.558260
714.798759	40707.895738	32.563277
715.300625	40772.781119	32.568295
715.787531	40848.010992	32.573312
716.521425	40901.493018	32.578330
717.038963	40983.313581	32.583348
718.032481	41047.677020	32.588365
719.459167	41108.934421	32.593383
719.756299	41179.635254	32.598400
720.797365	41250.867677	32.603418
721.629768	41316.591938	32.608436
722.488904	41375.098844	32.613453
723.117904	41443.369765	32.618471
723.637951	41511.573142	32.623488
724.854461	41558.599665	32.628506
725.173574	41630.528956	32.633524
725.887048	41694.081490	32.638541
726.733214	41752.563362	32.643559
727.120245	41818.962892	32.648576
728.015550	41897.911026	32.653594
728.920334	41951.413285	32.658612
729.443114	42025.374634	32.663629
730.534258	42098.504583	32.668647
730.912559	42162.127978	32.673664
731.820149	42222.503663	32.678682
732.697184	42286.044966	32.683700
733.076470	42353.116488	32.688717
734.151608	42412.336947	32.693735
734.810136	42485.266146	32.698752
735.492759	42564.834740	32.703770
736.262419	42622.237216	32.708788
737.137932	42675.806323	32.713805
737.691267	42747.901716	32.718823
738.424567	42827.750499	32.723840
739.655656	42876.942192	32.728858
740.136822	42941.917920	32.733876
740.608245	43019.191165	32.738893
741.436242	43077.005400	32.743911
742.018353	43138.196315	32.748928
742.713630	43206.050454	32.753946
743.476558	43289.129916	32.758964
744.345719	43362.262717	32.763981
745.129563	43421.063007	32.768999
745.553405	43497.730847	32.774016
746.412873	43558.453247	32.779034
747.440134	43617.660235	32.784052
747.846951	43683.770425	32.789069
748.638352	43743.482256	32.794087
749.392213	43812.004509	32.799104
749.778976	43867.213446	32.804122
750.625599	43949.292234	32.809140
751.261345	44007.566048	32.814157
752.142933	44070.583234	32.819175
752.544672	44145.030337	32.824192
753.346190	44207.950358	32.829210
753.970815	44288.028227	32.834228
754.412401	44370.529953	32.839245
755.155429	44443.192122	32.844263
756.174901	44532.186331	32.849280
757.036577	44608.167915	32.854298
758.069818	44681.254926	32.859316
759.001710	44753.194300	32.864333
759.684881	44832.757454	32.869351
760.135980	44904.578397	32.874368
761.148509	44972.101866	32.879386
762.040685	45051.238408	32.884404
762.809023	45126.924796	32.889421
763.713940	45197.255068	32.894439
764.416017	45266.091001	32.899456
765.125775	45339.323758	32.904474
765.783877	45421.171346	32.909492
766.588001	45487.673129	32.914509
767.707171	45550.279283	32.919527
768.278026	45639.814323	32.924544
768.936192	45712.343863	32.929562
769.696001	45786.223582	32.934580
770.190913	45863.846457	32.939597
771.273874	45941.294044	32.944615
771.823787	46031.761963	32.949632
772.498511	46105.741757	32.954650
773.652457	46181.087391	32.959668
774.072328	46253.452033	32.964685
775.118162	46329.254052	32.969703
775.562091	46432.988622	32.974720
776.359460	46504.275150	32.979738
777.587959	46577.070848	32.984756
778.288836	46666.959577	32.989773
779.268123	46739.454875	32.994791
779.946668	46805.858611	32.999808
780.751579	46889.806734	33.004826
781.537487	46963.712504	33.009844
782.609728	47023.646431	33.014861
783.452385	47104.683734	33.019879
783.787640	47181.385008	33.024896
784.586891	47258.533357	33.029914
785.897857	47323.645745	33.034932
785.944552	47407.836924	33.039949
787.062164	47481.701538	33.044967
788.042802	47566.435799	33.049984
788.722658	47619.215145	33.055002
789.847751	47685.481710	33.060020
790.296049	47751.240983	33.065037
791.069496	47812.676562	33.070055
791.934390	47877.376097	33.075072
792.557462	47937.917872	33.080090
793.686656	48002.339153	33.085108
794.100719	48082.997973	33.090125
794.866697	48136.055445	33.095143
795.758291	48204.118623	33.100160
796.246454	48277.335801	33.105178
797.141678	48354.713475	33.110196
797.822136	48431.936351	33.115213
798.803145	48497.124531	33.120231
799.519438	48576.178749	33.125248
800.173221	48651.292731	33.130266
801.215681	48729.459543	33.135284
801.869344	48800.453231	33.140301
802.396654	48871.126528	33.145319
802.988788	48944.093256	33.150336
803.907503	49038.367535	33.155354
804.918749	49120.712547	33.160372
805.391409	49201.446017	33.165389
806.223928	49277.736441	33.170407
806.942798	49375.767801	33.175424
808.029620	49467.591015	33.180442
809.025255	49539.726019	33.185460
809.648969	49625.328458	33.190477
810.684823	49706.845516	33.195495
811.508901	49791.662684	33.200512
812.037179	49879.433642	33.205530
813.269217	49956.654250	33.210548
813.864158	50048.268434	33.215565
814.482149	50124.697616	33.220583
815.364176	50203.773720	33.225600
816.240479	50306.332447	33.230618
817.395971	50380.572341	33.235636
818.114551	50472.364676	33.240653
819.121911	50542.892470	33.245671
819.649772	50628.265677	33.250688
820.309581	50721.551839	33.255706
821.259633	50802.465881	33.260724
822.006559	50884.646527	33.265741
823.157213	50958.899065	33.270759
823.939701	51051.356383	33.275776
824.618513	51139.939551	33.280794
825.969219	51217.639040	33.285812
826.325748	51309.171394	33.290829
827.137875	51380.806555	33.295847
827.957401	51466.525508	33.300864
828.747522	51554.865786	33.305882
830.055842	51627.161441	33.310900
830.612352	51711.140334	33.315917
831.361793	51797.001412	33.320935
832.239712	51874.469714	33.325952
832.883659	51965.375816	33.330970
834.181988	52030.053028	33.335988
834.967744	52102.866136	33.341005
835.898128	52155.158292	33.346023
836.302716	52234.985267	33.351040
837.172286	52314.672317	33.356058
838.277517	52377.778251	33.361076
838.996997	52458.528161	33.366093
839.858899	52533.208744	33.371111
840.632134	52602.225962	33.376128
841.299028	52678.787645	33.381146
842.225006	52750.779410	33.386164
842.829578	52834.194105	33.391181
843.464232	52913.978001	33.396199
844.399026	52997.927938	33.401216
845.036130	53084.497913	33.406234
846.001324	53175.453674	33.411252
846.478651	53264.174045	33.416269
847.821858	53346.195292	33.421287
848.411601	53431.764480	33.426304
849.153250	53526.516643	33.431322
850.310719	53613.650208	33.436340
850.930573	53711.601070	33.441357
851.683621	53800.826223	33.446375
852.572304	53898.602748	33.451392
853.208930	53997.685597	33.456410
854.499736	54093.824174	33.461428
854.991482	54184.809846	33.466445
855.927775	54275.876732	33.471463
856.929608	54372.523602	33.476480
857.893398	54464.518192	33.481498
858.897108	54556.494268	33.486516
860.047135	54656.278637	33.491533
860.656667	54753.908487	33.496551
861.921833	54834.108675	33.501568
862.411517	54917.162981	33.506586
863.552339	55006.884725	33.511604
864.164006	55101.924616	33.516621
864.819540	55190.345095	33.521639
866.077233	55276.381682	33.526656
866.687840	55387.237508	33.531674
867.836426	55467.724188	33.536692
868.781806	55569.234888	33.541709
869.298974	55655.728863	33.546727
870.072852	55741.948805	33.551744
870.851590	55851.660087	33.556762
871.986420	55928.988033	33.561780
872.607618	56032.481606	33.566797
873.707957	56133.711929	33.571815
874.787373	56227.789888	33.576832
875.454404	56319.241270	33.581850
876.341142	56411.595696	33.586868
877.307946	56497.406525	33.591885
878.311094	56592.947442	33.596903
879.384255	56681.756922	33.601920
880.066733	56772.671450	33.606938
880.945599	56858.494803	33.611956
881.524253	56948.779576	33.616973
882.211556	57024.999549	33.621991
883.368529	57107.190476	33.627008
883.793791	57204.076643	33.632026
884.671202	57287.209413	33.637044
886.074317	57372.263535	33.642061
886.686259	57457.810152	33.647079
887.614713	57552.490314	33.652096
888.438994	57645.204974	33.657114
889.552771	57729.378644	33.662132
890.656923	57815.192702	33.667149
891.148308	57918.067191	33.672167
892.201252	58003.741894	33.677184
892.934041	58092.587079	33.682202
893.983163	58180.990881	33.687220
894.692910	58275.763219	33.692237
895.770687	58359.648726	33.697255
896.914373	58454.760191	33.702272
897.433850	58555.840526	33.707290
898.211466	58637.290413	33.712308
899.284385	58737.838519	33.717325
899.862274	58844.230901	33.722343
901.134255	58938.784560	33.727360
901.656448	59041.332030	33.732378
902.664115	59140.206760	33.737396
903.796132	59239.520026	33.742413
904.600915	59329.240539	33.747431
905.663876	59427.684930	33.752448
906.411027	59529.454180	33.757466
907.330135	59627.417354	33.762484
908.765197	59718.147657	33.767501
909.271803	59829.555016	33.772519
910.238049	59917.844506	33.777536
911.090250	60014.778440	33.782554
911.937465	60119.894409	33.787572
913.005716	60217.827479	33.792589
914.054445	60320.048761	33.797607
915.179868	60419.640899	33.802624
916.112744	60503.016051	33.807642
917.068824	60597.533671	33.812660
918.004121	60691.458315	33.817677
918.740088	60785.604596	33.822695
919.932994	60881.765747	33.827712
920.722662	60978.503071	33.832730
921.507498	61078.250787	33.837748
922.474942	61171.045480	33.842765
923.269073	61273.391413	33.847783
924.146882	61366.229751	33.852800
925.001120	61472.574171	33.857818
926.239216	61564.547817	33.862836
927.380480	61660.061232	33.867853
927.998477	61757.745593	33.872871
929.069969	61862.709336	33.877888
929.675712	61957.987389	33.882906
930.374170	62041.179316	33.887924
931.237967	62126.934621	33.892941
932.158307	62227.639441	33.897959
933.137318	62312.297316	33.902976
933.938655	62398.894279	33.907994
934.860208	62497.794114	33.913012
936.091235	62596.926268	33.918029
936.589871	62694.053432	33.923047
937.607250	62787.296547	33.928064
938.583604	62893.329551	33.933082
939.302762	62987.211615	33.938100
940.426862	63095.953784	33.943117
941.145463	63203.043207	33.948135
942.221158	63299.964819	33.953152
942.848060	63407.733145	33.958170
944.117056	63503.166081	33.963188
945.157755	63609.322326	33.968205
945.957283	63711.746920	33.973223
947.612584	63806.523064	33.978240
948.680124	63904.775414	33.983258
949.441395	64010.258333	33.988276
950.381123	64102.171791	33.993293
951.436160	64196.562205	33.998311
952.524770	64293.189972	34.003328
953.324834	64396.729805	34.008346
954.140634	64491.251326	34.013364
955.574871	64597.022025	34.018381
956.189686	64706.546060	34.023399
956.984766	64792.362239	34.028416
958.036233	64899.657736	34.033434
958.631923	65002.987034	34.038452
959.966485	65102.428446	34.043469
960.453304	65214.530733	34.048487
962.068450	65313.641205	34.053504
962.725881	65412.977202	34.058522
963.680282	65534.677531	34.063540
964.812129	65630.790383	34.068557
965.327612	65732.216133	34.073575
966.613603	65844.236011	34.078592
967.820262	65953.609842	34.083610
968.028614	66054.252353	34.088628
968.985617	66165.284186	34.093645
970.067480	66281.018589	34.098663
971.037425	66393.458321	34.103680
972.105726	66514.950911	34.108698
972.758336	66619.208421	34.113716
974.119235	66733.315608	34.118733
975.141383	66854.388128	34.123751
975.977060	66961.625241	34.128768
977.208964	67070.556049	34.133786
978.077312	67186.355121	34.138804
979.282113	67292.543563	34.143821
979.984487	67410.379222	34.148839
981.090324	67510.317991	34.153856
981.854660	67623.824136	34.158874
983.012315	67732.960003	34.163892
984.121321	67833.695910	34.168909
984.692809	67932.527898	34.173927
985.862846	68027.885381	34.178944
987.000775	68128.681392	34.183962
987.786598	68236.243041	34.188980
988.653252	68339.907192	34.193997
989.351643	68444.104062	34.199015
990.507764	68544.558191	34.204032
991.757797	68657.121287	34.209050
992.691009	68769.906010	34.214068
993.859202	68870.025067	34.219085
994.488369	68987.755579	34.224103
995.526664	69091.421693	34.229120
996.911248	69189.789554	34.234138
998.072584	69302.212542	34.239156
999.193637	69401.577376	34.244173
999.823263	69514.951711	34.249191
1001.199512	69618.611086	34.254208
1002.179673	69716.572097	34.259226
1002.947224	69826.034467	34.264244
1004.272920	69906.908319	34.269261
1005.247834	70025.209232	34.274279
1006.306334	70136.693038	34.279296
1007.311003	70242.051196	34.284314
1007.949014	70343.405708	34.289332
1009.433806	70445.794892	34.294349
1010.150651	70551.863902	34.299367
1011.668392	70671.693490	34.304384
1012.718261	70779.663078	34.309402
1013.437036	70882.220620	34.314420
1014.490205	70983.360748	34.319437
1015.594121	71088.537059	34.324455
1016.088680	71201.633012	34.329472
1017.304795	71306.072340	34.334490
1018.625698	71412.353174	34.339508
1019.153098	71530.683776	34.344525
1020.053978	71641.512461	34.349543
1021.544391	71744.255023	34.354560
1022.411635	71870.867765	34.359578
1022.654122	71990.383781	34.364596
1024.114509	72098.516430	34.369613
1025.017843	72222.364422	34.374631
1025.929062	72331.185974	34.379648
1027.644635	72449.301462	34.384666
1028.317724	72581.067828	34.389684
1029.569491	72691.593815	34.394701
1030.637635	72811.027662	34.399719
1031.417213	72915.519642	34.404736
1032.367760	73024.130209	34.409754
1033.078947	73154.428312	34.414772
1034.540633	73265.107346	34.419789
1035.609025	73383.615689	34.424807
1036.166356	73516.019600	34.429824
1037.937124	73626.708349	34.434842
1038.683790	73739.134090	34.439860
1039.841261	73838.869327	34.444877
1040.635668	73946.315419	34.449895
1041.825175	74046.343600	34.454912
1042.985416	74146.869844	34.459930
1043.158386	74266.151461	34.464948
1044.285268	74371.524758	34.469965
1045.562556	74491.820103	34.474983
1046.138679	74611.273462	34.480000
1047.541720	74723.315944	34.485018
1048.705140	74843.821096	34.490036
1049.595112	74958.543827	34.495053
1050.930751	75077.007043	34.500071
1051.876992	75201.643987	34.505088
1053.034819	75316.477825	34.510106
1053.810466	75444.448596	34.515124
1055.157227	75556.018053	34.520141
1056.279054	75676.016584	34.525159
1056.985050	75783.511838	34.530176
1058.227602	75910.918355	34.535194
1059.330950	76041.040096	34.540212
1060.189115	76161.443682	34.545229
1061.311751	76284.611988	34.550247
1062.522887	76410.257053	34.555264
1063.956978	76532.385085	34.560282
1064.731265	76660.673450	34.565300
1065.613141	76777.341747	34.570317
1066.870573	76902.729696	34.575335
1067.589696	77034.303043	34.580352
1068.811660	77161.556373	34.585370
1069.843829	77289.068217	34.590388
1070.989667	77412.441925	34.595405
1072.054091	77548.577516	34.600423
1073.319501	77672.483653	34.605440
1074.537591	77797.662160	34.610458
1075.497128	77928.394024	34.615476
1076.432221	78047.974881	34.620493
1077.644432	78169.749841	34.625511
1078.836776	78307.431324	34.630528
1079.835036	78423.420547	34.635546
1081.119817	78557.650583	34.640564
1082.561649	78676.414998	34.645581
1083.550495	78804.859698	34.650599
1084.593755	78923.176953	34.655616
1085.840395	79034.933125	34.660634
1086.715355	79162.936759	34.665652
1087.946910	79293.874264	34.670669
1089.178637	79413.447512	34.675687
1090.334432	79526.339613	34.680704
1091.050900	79642.999999	34.685722
1091.904073	79780.587280	34.690740
1093.152881	79899.680234	34.695757
1094.295876	80022.134584	34.700775
1095.502309	80147.993003	34.705792
1096.669119	80262.827984	34.710810
1097.490773	80372.832179	34.715828
1098.625268	80485.359962	34.720845
1099.659905	80604.579541	34.725863
1100.652858	80721.454895	34.730880
1101.794160	80825.569737	34.735898
1102.739208	80949.540261	34.740916
1103.683499	81061.071031	34.745933
1105.085463	81183.781855	34.750951
1105.708210	81311.548119	34.755968
1107.172615	81430.546058	34.760986
1108.241767	81550.119588	34.766004
1109.214154	81679.103143	34.771021
1110.589041	81797.813982	34.776039
1111.541073	81923.053534	34.781056
1112.709827	82042.595085	34.786074
1113.765022	82166.700744	34.791092
1114.982242	82296.907219	34.796109
1116.390161	82410.173203	34.801127
1117.257163	82548.105353	34.806144
1118.743617	82662.340109	34.811162
1119.710269	82785.926161	34.816180
1120.656987	82907.581578	34.821197
1121.853535	83034.596996	34.826215
1122.478594	83159.617781	34.831232
1124.023864	83291.776051	34.836250
1124.817591	83436.344959	34.841268
1125.975836	83563.350701	34.846285
1127.200266	83689.619626	34.851303
1128.051226	83840.852177	34.856320
1129.730896	83949.379478	34.861338
1130.572572	84099.869330	34.866356
1131.820541	84236.911104	34.871373
1133.424823	84358.350214	34.876391
1134.111010	84497.183753	34.881408
1135.437434	84625.452612	34.886426
1136.473168	84762.038386	34.891444
1137.484566	84890.997531	34.896461
1138.961283	85025.921585	34.901479
1139.977533	85168.582815	34.906496
1141.378918	85289.711791	34.911514
1142.238099	85429.883312	34.916532
1143.440026	85555.876115	34.921549
1144.552409	85688.339522	34.926567
1145.544023	85833.158895	34.931584
1146.967445	85963.658720	34.936602
1148.318617	86099.779300	34.941620
1149.325846	86220.369252	34.946637
1150.532571	86349.091198	34.951655
1151.385907	86488.328478	34.956672
1152.831793	86614.573286	34.961690
1154.360840	86751.491741	34.966708
1155.213707	86878.496339	34.971725
1156.544132	87006.001164	34.976743
1157.513088	87127.797410	34.981760
1158.947426	87261.755933	34.986778
1160.156311	87377.457722	34.991796
1161.147871	87500.915530	34.996813
1162.497292	87610.247561	35.001831
1163.304575	87732.205736	35.006848
1164.473427	87829.477180	35.011866
1165.729594	87954.628148	35.016884
1166.767564	88068.438489	35.021901
1168.111077	88177.540374	35.026919
1168.910357	88305.497814	35.031936
1170.327550	88425.440553	35.036954
1171.630198	88548.899168	35.041972
1172.810333	88662.588859	35.046989
1174.037962	88782.873589	35.052007
1174.598504	88906.515487	35.057024
1175.849104	89033.456903	35.062042
1177.143357	89169.726139	35.067060
1178.076206	89296.390780	35.072077
1179.343903	89422.838495	35.077095
1180.432420	89548.056966	35.082112
1181.672015	89681.252009	35.087130
1182.781579	89822.234475	35.092148
1183.716525	89962.486730	35.097165
1185.466523	90098.569169	35.102183
1186.394382	90229.799738	35.107200
1187.856681	90370.767614	35.112218
1188.724390	90510.287825	35.117236
1190.262118	90640.298175	35.122253
1191.283268	90772.491112	35.127271
1192.452262	90899.639795	35.132288
1193.778240	91042.537314	35.137306
1194.908273	91184.840800	35.142324
1196.151115	91325.710588	35.147341
1197.480657	91459.559923	35.152359
1198.372277	91603.162609	35.157376
1199.768796	91739.482230	35.162394
1201.287314	91870.356756	35.167412
1202.296676	92017.459927	35.172429
1203.777739	92152.554326	35.177447
1205.061775	92289.293695	35.182464
1206.469684	92409.708887	35.187482
1207.866431	92539.019225	35.192500
1208.934699	92677.370188	35.197517
1210.139146	92794.979964	35.202535
1211.422447	92939.737136	35.207552
1212.608670	93056.541607	35.212570
1213.934966	93185.063652	35.217588
1214.758562	93321.193184	35.222605
1216.116157	93454.911014	35.227623
1217.072023	93591.704285	35.232640
1218.627801	93720.268847	35.237658
1219.711841	93851.572067	35.242676
1221.063760	93998.305024	35.247693
1222.251391	94113.735929	35.252711
1223.319960	94259.250598	35.257728
1224.460113	94387.878772	35.262746
1225.930661	94499.098282	35.267764
1226.692296	94627.155475	35.272781
1227.902766	94751.372068	35.277799
1229.304965	94875.267895	35.282816
1230.446046	94992.058074	35.287834
1231.842563	95116.563392	35.292852
1232.497684	95241.490903	35.297869
1233.903745	95360.233438	35.302887
1234.878073	95500.824520	35.307904
1236.174487	95628.587340	35.312922
1237.288561	95761.029299	35.317940
1238.456576	95907.038596	35.322957
1239.811592	96040.734356	35.327975
1240.586303	96183.765253	35.332992
1242.171653	96321.803560	35.338010
1243.200378	96465.466405	35.343028
1244.108388	96613.843234	35.348045
1246.118062	96755.017681	35.353063
1246.722567	96910.352724	35.358080
1248.248188	97062.284447	35.363098
1249.605486	97197.637806	35.368116
1250.683347	97344.297010	35.373133
1252.448138	97492.201768	35.378151
1253.617695	97641.049839	35.383168
1254.981305	97781.163031	35.388186
1256.535013	97922.872737	35.393204
1257.851915	98065.734416	35.398221
1259.132805	98216.770135	35.403239
1260.312791	98365.387204	35.408256
1261.560700	98505.788957	35.413274
1262.916938	98649.160483	35.418292
1264.097641	98793.035308	35.423309
1265.374568	98926.659257	35.428327
1266.961515	99082.567832	35.433344
1267.942617	99215.164958	35.438362
1269.688240	99352.879856	35.443380
1270.438176	99506.520210	35.448397
1272.152181	99635.257796	35.453415
1273.183102	99785.888069	35.458432
1274.554480	99939.318639	35.463450
1275.762973	100067.253237	35.468468
1276.872142	100203.967196	35.473485
1278.304481	100360.408846	35.478503
1279.652722	100498.851785	35.483520
1280.865102	100645.112133	35.488538
1281.994520	100783.401748	35.493556
1283.379273	100939.000715	35.498573
1285.122146	101081.212349	35.503591
1286.432451	101230.826909	35.508608
1287.388208	101381.023959	35.513626
1288.746750	101509.581737	35.518644
1290.077173	101656.626945	35.523661
1291.579418	101791.566741	35.528679
1292.894099	101939.609642	35.533696
1293.977098	102073.504085	35.538714
1295.191120	102210.067665	35.543732
1296.042682	102341.209995	35.548749
1297.683377	102455.902435	35.553767
1298.963516	102585.813735	35.558784
1300.187890	102734.622692	35.563802
1301.551242	102856.726588	35.568820
1302.528945	102985.618800	35.573837
1303.454783	103125.631526	35.578855
1304.656483	103272.960477	35.583872
1306.019239	103411.519665	35.588890
1307.376982	103556.458976	35.593908
1308.408444	103701.780094	35.598925
1309.983866	103850.616256	35.603943
1311.533029	103997.793268	35.608960
1312.587525	104143.556408	35.613978
1313.994200	104298.661671	35.618996
1315.242026	104453.647655	35.624013
1316.543465	104596.760822	35.629031
1318.003995	104756.391492	35.634048
1319.516777	104903.124292	35.639066
1320.767807	105046.532960	35.644084
1321.876192	105198.685595	35.649101
1323.359612	105357.164913	35.654119
1324.748647	105511.945515	35.659136
1325.721734	105674.741768	35.664154
1327.578909	105812.464360	35.669172
1328.705459	105977.434272	35.674189
1330.517925	106134.050170	35.679207
1332.028340	106282.127179	35.684224
1333.071228	106438.323131	35.689242
1334.782485	106570.061069	35.694260
1335.883769	106726.357205	35.699277
1337.295016	106873.086626	35.704295
1338.595970	107026.580981	35.709312
1340.186079	107179.758218	35.714330
1341.429361	107317.890836	35.719348
1342.606103	107465.218087	35.724365
1344.337393	107616.957990	35.729383
1345.693873	107766.935669	35.734400
1346.766471	107930.313679	35.739418
1348.423505	108063.372205	35.744436
1349.431180	108216.167590	35.749453
1351.051242	108358.853881	35.754471
1352.546022	108507.472393	35.759488
1353.753962	108658.472893	35.764506
1355.238880	108799.170561	35.769524
1356.599725	108938.382390	35.774541
1358.088223	109093.524677	35.779559
1359.390268	109237.032529	35.784576
1360.623272	109387.938636	35.789594
1362.488039	109539.099720	35.794612
1363.596295	109675.311437	35.799629
1364.930557	109815.304702	35.804647
1365.988113	109964.577592	35.809664
1367.531289	110106.412875	35.814682
1368.924020	110245.829649	35.819700
1369.961755	110392.361230	35.824717
1371.393228	110517.094860	35.829735
1372.623370	110647.747786	35.834752
1373.689876	110792.852992	35.839770
1375.146742	110933.681354	35.844788
1376.384507	111075.140349	35.849805
1377.454652	111221.595764	35.854823
1378.904926	111360.091881	35.859840
1379.654910	111520.316916	35.864858
1381.312871	111669.979489	35.869876
1382.644371	111817.548965	35.874893
1384.211264	111978.894164	35.879911
1385.612764	112135.044342	35.884928
1386.877953	112293.958129	35.889946
1388.202254	112456.864233	35.894964
1389.558609	112634.408190	35.899981
1391.169027	112788.788457	35.904999
1392.657470	112945.271748	35.910016
1393.903820	113110.543074	35.915034
1395.386594	113268.232064	35.920052
1396.541912	113446.339178	35.925069
1398.279728	113605.445773	35.930087
1399.807239	113769.771517	35.935104
1401.151983	113946.522672	35.940122
1402.547664	114108.687536	35.945140
1403.944854	114280.982281	35.950157
1405.065993	114442.236994	35.955175
1407.025630	114601.833781	35.960192
1408.151378	114776.593404	35.965210
1409.323544	114957.861297	35.970228
1410.790962	115121.755938	35.975245
1412.487929	115293.497167	35.980263
1413.950802	115456.280458	35.985280
1414.903350	115631.491358	35.990298
1416.950082	115801.863606	35.995316
1418.586419	115980.095795	36.000333
1419.574271	116152.677277	36.005351
1421.262074	116306.889576	36.010368
1422.969115	116485.272351	36.015386
1424.664098	116658.416003	36.020404
1426.491941	116813.698097	36.025421
1427.877728	116965.892042	36.030439
1430.067226	117103.688256	36.035456
1430.821296	117274.339084	36.040474
1432.044360	117429.638715	36.045492
1433.643802	117577.946493	36.050509
1434.730756	117735.650246	36.055527
1436.628747	117878.441879	36.060544
1437.619050	118051.257386	36.065562
1439.215931	118206.654273	36.070580
1440.852893	118360.842710	36.075597
1442.374778	118524.585931	36.080615
1443.655463	118687.570715	36.085632
1444.561098	118837.553610	36.090650
1446.170080	118982.809705	36.095668
1447.558999	119126.259008	36.100685
1448.656764	119272.731365	36.105703
1450.438063	119432.139745	36.110720
1451.540612	119578.220485	36.115738
1452.862646	119714.028299	36.120756
1454.431360	119886.992105	36.125773
1455.433618	120035.104939	36.130791
1457.125004	120195.786042	36.135808
1458.134104	120354.018347	36.140826
1459.703802	120521.255589	36.145844
1461.113525	120693.534463	36.150861
1462.425515	120865.171440	36.155879
1464.231293	121034.894705	36.160896
1465.515500	121200.953175	36.165914
1466.746718	121368.604217	36.170932
1468.200068	121543.085415	36.175949
1469.569871	121730.752645	36.180967
1471.246794	121898.766855	36.185984
1472.592110	122083.299541	36.191002
1474.351714	122257.508833	36.196020
1475.885137	122440.354975	36.201037
1477.209088	122630.682935	36.206055
1478.993625	122801.928135	36.211072
1480.387575	122981.709784	36.216090
1482.080121	123162.230480	36.221108
1483.705405	123338.697374	36.226125
1485.071973	123521.615465	36.231143
1486.930387	123684.621805	36.236160
1488.586879	123864.114376	36.241178
1489.999615	124034.197968	36.246196
1491.695757	124200.171771	36.251213
1492.983803	124385.033502	36.256231
1494.558434	124551.674765	36.261248
1495.943557	124727.745657	36.266266
1497.552110	124889.545052	36.271284
1498.799268	125065.779406	36.276301
1500.249993	125256.599908	36.281319
1502.465208	125416.241415	36.286336
1503.784728	125596.989771	36.291354
1505.430232	125776.116846	36.296372
1507.019526	125941.244337	36.301389
1508.179614	126121.210831	36.306407
1509.873541	126289.059904	36.311424
1511.323486	126465.765173	36.316442
1512.974504	126637.930079	36.321460
1514.639011	126807.053756	36.326477
1516.187955	126991.955184	36.331495
1517.770671	127152.999479	36.336512
1519.129328	127317.487911	36.341530
1520.559046	127496.483240	36.346548
1522.304876	127674.618780	36.351565
1523.520176	127830.683648	36.356583
1525.185087	128001.892176	36.361600
1526.395841	128176.670295	36.366618
1527.958546	128335.368458	36.371636
1529.640764	128493.465813	36.376653
1530.861280	128651.662758	36.381671
1532.230517	128806.543221	36.386688
1533.545223	128970.896501	36.391706
1534.903443	129142.515544	36.396724
1536.850124	129300.043425	36.401741
1538.214719	129474.463258	36.406759
1539.369252	129636.020821	36.411776
1540.918560	129804.104369	36.416794
1542.580153	129980.076457	36.421812
1544.360050	130162.884755	36.426829
1545.887752	130336.511271	36.431847
1547.495847	130503.094751	36.436864
1548.857534	130687.062455	36.441882
1550.147944	130862.452936	36.446900
1551.701689	131051.308189	36.451917
1553.117872	131232.787623	36.456935
1555.052532	131430.668889	36.461952
1556.270458	131606.823028	36.466970
1557.962951	131791.492914	36.471988
1559.562025	131985.009665	36.477005
1560.879347	132176.241245	36.482023
1562.716864	132367.049396	36.487040
1564.184645	132555.522932	36.492058
1565.820999	132759.048355	36.497076
1567.505064	132928.776281	36.502093
1569.097601	133134.249885	36.507111
1570.624416	133319.614889	36.512128
1572.233730	133509.035201	36.517146
1573.810250	133714.680242	36.522164
1575.635228	133904.309654	36.527181
1577.314783	134107.128271	36.532199
1579.045449	134300.158358	36.537216
1580.726727	134491.753108	36.542234
1582.135190	134684.203408	36.547252
1583.525741	134867.217918	36.552269
1585.214994	135056.128894	36.557287
1586.986109	135243.875024	36.562304
1588.904876	135448.654462	36.567322
1590.326547	135634.266495	36.572340
1592.027182	135820.963165	36.577357
1593.470243	136018.890906	36.582375
1595.169336	136199.305170	36.587392
1596.541323	136388.338570	36.592410
1598.077648	136588.358864	36.597428
1599.937112	136786.466438	36.602445
1601.650762	136977.844364	36.607463
1603.365893	137160.188150	36.612480
1604.801194	137357.669995	36.617498
1606.554228	137545.319767	36.622516
1608.228028	137726.482446	36.627533
1610.001256	137924.560707	36.632551
1611.387184	138105.137817	36.637568
1613.283745	138287.675202	36.642586
1614.466023	138451.723809	36.647604
1616.263210	138617.361122	36.652621
1617.712891	138785.221589	36.657639
1619.390033	138959.687423	36.662656
1620.614808	139123.352808	36.667674
1622.368058	139297.364984	36.672692
1623.995799	139472.310568	36.677709
1625.436971	139648.237290	36.682727
1627.065330	139819.826443	36.687744
1628.960001	140000.625745	36.692762
1630.268975	140203.798852	36.697780
1631.814587	140367.432765	36.702797
1633.208340	140560.113924	36.707815
1634.781391	140745.531242	36.712832
1636.377336	140947.801994	36.717850
1638.089779	141142.400674	36.722868
1639.782749	141336.129207	36.727885
1641.271651	141538.699736	36.732903
1642.516555	141739.852862	36.737920
1644.172366	141945.910289	36.742938
1645.730073	142144.240795	36.747956
1647.846826	142345.246787	36.752973
1649.554173	142562.085958	36.757991
1650.937442	142762.273285	36.763008
1652.838452	142973.748700	36.768026
1654.247850	143180.956273	36.773044
1656.371447	143393.539945	36.778061
1658.279371	143599.010786	36.783079
1660.043217	143791.919789	36.788096
1661.524313	144001.732512	36.793114
1663.169563	144203.079051	36.798132
1665.137598	144400.813948	36.803149
1667.135466	144618.572102	36.808167
1668.419936	144824.124744	36.813184
1670.373060	145016.022646	36.818202
1672.078427	145211.510187	36.823220
1674.387789	145410.654977	36.828237
1675.707926	145611.327089	36.833255
1677.479935	145797.212321	36.838272
1679.164117	145982.111222	36.843290
1680.287974	146191.577131	36.848308
1682.670096	146377.559053	36.853325
1684.265399	146581.755592	36.858343
1685.841587	146788.871974	36.863360
1687.506770	146971.688163	36.868378
1689.072373	147189.938473	36.873396
1690.719372	147385.474160	36.878413
1692.299244	147593.343121	36.883431
1693.743816	147785.211920	36.888448
1695.761564	148002.736844	36.893466
1697.165462	148214.073136	36.898484
1699.071969	148411.475407	36.903501
1700.996561	148613.807283	36.908519
1702.645309	148818.732283	36.913536
1704.254695	149008.820178	36.918554
1705.699429	149197.553550	36.923572
1707.775711	149375.120677	36.928589
1709.688877	149565.163622	36.933607
1710.785480	149748.681817	36.938624
1712.749899	149915.164455	36.943642
1714.080989	150112.922086	36.948660
1715.929655	150297.135321	36.953677
1717.581495	150491.472136	36.958695
1718.702391	150684.246335	36.963712
1720.564859	150873.734513	36.968730
1722.253354	151089.012538	36.973748
1724.210222	151280.871504	36.978765
1725.628335	151488.563058	36.983783
1727.204302	151696.205507	36.988800
1729.217338	151896.857664	36.993818
1730.720673	152115.252588	36.998836
1732.582837	152317.896376	37.003853
1734.230867	152527.662563	37.008871
1736.164528	152754.969612	37.013888
1737.891684	152971.623079	37.018906
1739.358986	153194.468306	37.023924
1741.458927	153399.147556	37.028941
1743.495829	153621.753062	37.033959
1744.964971	153843.778224	37.038976
1746.773082	154057.839433	37.043994
1748.442172	154272.012835	37.049012
1750.213223	154495.097447	37.054029
1752.095267	154714.032528	37.059047
1753.640504	154932.109607	37.064064
1755.817219	155142.581710	37.069082
1757.258556	155367.829204	37.074100
1759.425525	155580.118726	37.079117
1761.499319	155785.792988	37.084135
1763.124412	155991.146669	37.089152
1765.019109	156206.120686	37.094170
1766.691428	156418.265742	37.099188
1768.567559	156627.907194	37.104205
1770.472890	156839.941795	37.109223
1772.435700	157057.497052	37.114240
1774.441231	157273.119537	37.119258
1775.516641	157498.350423	37.124276
1777.678881	157707.103472	37.129293
1779.677523	157912.789766	37.134311
1781.226363	158129.048038	37.139328
1783.283989	158342.373784	37.144346
1784.888145	158563.114858	37.149364
1786.979553	158757.657936	37.154381
1788.560756	158976.591950	37.159399
1790.242685	159182.120468	37.164416
1792.335042	159387.166570	37.169434
1793.928423	159615.093353	37.174452
1795.621766	159821.460750	37.179469
1797.625862	160026.778221	37.184487
1799.219001	160248.343256	37.189504
1801.412035	160442.752743	37.194522
1803.406854	160631.196525	37.199540
1804.380922	160825.205606	37.204557
1806.286512	161020.285284	37.209575
1807.742451	161234.269419	37.214592
1809.429716	161428.384156	37.219610
1811.139355	161638.969833	37.224628
1813.060299	161832.073184	37.229645
1814.767568	162045.083834	37.234663
1816.145675	162260.938008	37.239680
1818.099579	162465.123476	37.244698
1819.652834	162678.542786	37.249716
1821.607998	162897.682584	37.254733
1823.193880	163118.290050	37.259751
1825.007863	163346.953914	37.264768
1827.010663	163559.926594	37.269786
1828.661709	163790.052212	37.274804
1830.504379	164019.502059	37.279821
1832.568193	164235.880590	37.284839
1833.567503	164471.567450	37.289856
1835.917968	164708.055960	37.294874
1837.664407	164944.870164	37.299892
1839.301435	165181.538382	37.304909
1842.039891	165421.444994	37.309927
1843.578783	165663.927987	37.314944
1845.257922	165892.857423	37.319962
1847.029084	166140.278437	37.324980
1849.215590	166367.608278	37.329997
1851.656194	166610.322125	37.335015
1853.231614	166852.971945	37.340032
1855.639183	167081.209613	37.345050
1857.310568	167312.191025	37.350068
1859.463091	167540.928578	37.355085
1861.321972	167779.467927	37.360103
1863.170762	168011.579685	37.365120
1865.179264	168228.040951	37.370138
1866.812387	168464.350029	37.375156
1868.632943	168698.335011	37.380173
1870.807037	168914.583641	37.385191
1872.480845	169155.888093	37.390208
1874.269908	169389.222726	37.395226
1876.588977	169623.464034	37.400244
1878.331738	169846.838892	37.405261
1880.336320	170078.316941	37.410279
1882.192809	170313.498412	37.415296
1884.089897	170539.440435	37.420314
1885.989358	170766.804088	37.425332
1887.659052	170997.249892	37.430349
1890.036914	171231.085688	37.435367
1891.344666	171465.929935	37.440384
1893.554297	171697.334340	37.445402
1895.458012	171919.718811	37.450420
1897.592870	172155.704424	37.455437
1899.351391	172376.173686	37.460455
1901.072508	172620.397047	37.465472
1903.340951	172837.578564	37.470490
1904.943248	173044.883532	37.475508
1906.650278	173244.650438	37.480525
1909.003408	173442.501767	37.485543
1910.241845	173657.681996	37.490560
1912.278353	173859.606997	37.495578
1914.264236	174070.497218	37.500596
1916.132417	174285.631618	37.505613
1917.941232	174493.735901	37.510631
1919.723880	174716.649963	37.515648
1921.669161	174927.043674	37.520666
1923.293508	175163.495976	37.525684
1924.856064	175383.518140	37.530701
1927.045359	175606.829263	37.535719
1929.076073	175845.935902	37.540736
1930.977076	176066.415492	37.545754
1932.714325	176305.533329	37.550772
1934.502706	176538.745192	37.555789
1936.971978	176780.363052	37.560807
1938.753719	177020.619777	37.565824
1940.913430	177263.621695	37.570842
1942.980752	177488.040772	37.575860
1944.856891	177729.720239	37.580877
1947.067057	177968.595022	37.585895
1948.839153	178208.136982	37.590912
1950.792421	178440.090025	37.595930
1952.523714	178675.593933	37.600948
1954.529406	178924.009328	37.605965
1956.584189	179156.571889	37.610983
1958.456660	179419.056237	37.616000
1960.595533	179656.201048	37.621018
1962.908193	179896.986313	37.626036
1964.600021	180135.308552	37.631053
1966.654944	180373.511064	37.636071
1968.814840	180627.545289	37.641088
1970.611671	180863.063599	37.646106
1972.987617	181107.169846	37.651124
1974.901128	181343.941061	37.656141
1976.754229	181583.933238	37.661159
1978.628455	181824.316723	37.666176
1980.995808	182067.363940	37.671194
1983.116101	182309.601601	37.676212
1984.979763	182556.804406	37.681229
1987.617891	182789.255965	37.686247
1989.182470	183026.751479	37.691264
1991.115877	183254.914414	37.696282
1993.268945	183493.181881	37.701300
1995.244250	183730.768270	37.706317
1997.313833	183966.196571	37.711335
1999.086561	184210.238175	37.716352
2001.463481	184440.620818	37.721370
2003.505558	184674.940599	37.726388
2004.998261	184909.006168	37.731405
2007.651592	185133.993749	37.736423
2009.668685	185369.602711	37.741440
2011.391771	185602.620191	37.746458
2013.366939	185815.955867	37.751476
2015.463471	186014.744001	37.756493
2017.066103	186231.846020	37.761511
2019.036895	186452.570599	37.766528
2020.870065	186665.882024	37.771546
2023.167190	186872.763353	37.776564
2024.558168	187105.092506	37.781581
2026.815102	187310.725908	37.786599
2028.578833	187549.749071	37.791616
2030.270394	187777.402149	37.796634
2032.540302	188010.839997	37.801652
2034.328283	188244.368166	37.806669
2036.637619	188469.845462	37.811687
2038.507502	188716.941302	37.816704
2040.594860	188963.255220	37.821722
2042.963202	189201.594469	37.826740
2044.634265	189448.776451	37.831757
2047.028592	189683.344996	37.836775
2049.030527	189931.060751	37.841792
2051.184245	190171.723198	37.846810
2053.288725	190416.696756	37.851828
2055.391652	190669.679576	37.856845
2057.575570	190900.861022	37.861863
2059.607715	191152.867740	37.866880
2061.899775	191400.240472	37.871898
2063.928318	191634.153213	37.876916
2066.033419	191889.718314	37.881933
2068.107921	192120.719882	37.886951
2070.200251	192377.685568	37.891968
2072.169612	192625.509132	37.896986
2074.848926	192854.349559	37.902004
2076.794772	193091.835906	37.907021
2078.962493	193338.781273	37.912039
2081.034505	193581.351846	37.917056
2082.956547	193828.897041	37.922074
2085.415479	194059.465948	37.927092
2087.628138	194321.372294	37.932109
2089.580070	194553.051913	37.937127
2091.835849	194801.424684	37.942144
2093.842577	195043.593860	37.947162
2096.325912	195276.118992	37.952180
2098.189674	195518.287728	37.957197
2100.382034	195744.032950	37.962215
2102.671732	195987.392841	37.967232
2104.853431	196232.522516	37.972250
2107.417132	196455.089731	37.977268
2109.303954	196681.255612	37.982285
2111.663995	196917.932689	37.987303
2113.854915	197144.344272	37.992320
2115.740964	197367.467130	37.997338
2117.988903	197589.188149	38.002356
2120.227787	197812.231554	38.007373
2122.334213	198029.229928	38.012391
2124.349190	198263.378576	38.017408
2126.153507	198479.144780	38.022426
2128.778398	198670.069209	38.027444
2130.547595	198888.063853	38.032461
2132.859462	199083.088376	38.037479
2134.793917	199275.660313	38.042496
2136.756492	199472.391719	38.047514
2138.960877	199667.219644	38.052532
2141.075989	199881.495240	38.057549
2143.224152	200082.502329	38.062567
2144.811520	200289.729824	38.067584
2146.854502	200510.023131	38.072602
2148.983041	200712.254199	38.077620
2150.917883	200938.252890	38.082637
2153.176685	201158.159176	38.087655
2155.236639	201380.979246	38.092672
2157.207583	201608.498159	38.097690
2159.511399	201843.860469	38.102708
2161.459349	202083.265948	38.107725
2163.598846	202307.892292	38.112743
2165.842572	202552.228707	38.117760
2167.563023	202793.780438	38.122778
2170.039218	203013.126470	38.127796
2172.188209	203273.436913	38.132813
2174.559512	203516.005557	38.137831
2177.216765	203768.431031	38.142848
2179.441636	204001.821993	38.147866
2181.477574	204231.765751	38.152884
2184.144763	204475.586333	38.157901
2186.289616	204715.111367	38.162919
2188.116833	204944.887978	38.167936
2190.985298	205191.815096	38.172954
2193.044853	205431.128130	38.177972
2195.242171	205662.435653	38.182989
2197.665421	205899.864968	38.188007
2199.901172	206147.226527	38.193024
2201.918272	206374.427102	38.198042
2204.495795	206606.414319	38.203060
2206.370729	206851.551061	38.208077
2208.949452	207073.130472	38.213095
2211.620659	207307.987223	38.218112
2213.532782	207550.543948	38.223130
2215.872963	207770.373835	38.228148
2218.220134	207998.378794	38.233165
2220.488993	208230.408567	38.238183
2222.857582	208457.256638	38.243200
2225.099103	208680.964692	38.248218
2227.387120	208913.451046	38.253236
2229.185698	209135.161738	38.258253
2231.451178	209365.127088	38.263271
2233.779927	209598.409356	38.268288
2235.672467	209844.964543	38.273306
2238.037802	210069.064247	38.278324
2240.239308	210303.930840	38.283341
2242.597619	210544.410120	38.288359
2244.857109	210779.447032	38.293376
2246.857291	210999.697827	38.298394
2249.157534	211203.651770	38.303412
2250.975630	211416.836193	38.308429
2252.902860	211630.549927	38.313447
2255.229872	211842.118927	38.318464
2256.818061	212065.841121	38.323482
2259.751446	212271.589711	38.328500
2261.978096	212504.467247	38.333517
2263.529401	212737.440010	38.338535
2265.606231	212962.344690	38.343552
2267.889183	213199.240318	38.348570
2270.275618	213434.673076	38.353588
2272.186815	213674.993748	38.358605
2274.254449	213935.248398	38.363623
2276.861533	214176.400044	38.368640
2278.810901	214433.247498	38.373658
2281.322250	214678.656593	38.378676
2283.576084	214935.152990	38.383693
2286.049583	215198.763443	38.388711
2288.362961	215444.371765	38.393728
2290.705822	215703.370794	38.398746
2293.032761	215960.367323	38.403764
2295.288987	216223.533731	38.408781
2297.228633	216486.814820	38.413799
2299.707091	216750.798657	38.418816
2302.136688	217023.399434	38.423834
2304.476250	217294.644328	38.428852
2307.015340	217551.803561	38.433869
2309.784201	217820.176482	38.438887
2311.959977	218085.305236	38.443904
2314.365614	218357.762611	38.448922
2316.718330	218609.419471	38.453940
2319.155463	218884.819498	38.458957
2321.527649	219148.905304	38.463975
2324.107061	219394.764604	38.468992
2326.274479	219661.703443	38.474010
2328.580131	219925.739129	38.479028
2331.156308	220187.320444	38.484045
2333.591632	220440.925875	38.489063
2335.907251	220720.008823	38.494080
2338.166872	220975.446919	38.499098
2340.959579	221236.159584	38.504116
2343.218362	221490.507607	38.509133
2345.237053	221768.663835	38.514151
2347.814002	222013.986203	38.519168
2350.068542	222294.913066	38.524186
2352.336235	222544.742934	38.529204
2354.493502	222809.078896	38.534221
2356.822883	223090.352316	38.539239
2359.301335	223349.864944	38.544256
2361.522689	223620.859700	38.549274
2364.149141	223939.559621	38.554292
2366.939174	224218.910198	38.559309
2368.642425	224480.746123	38.564327
2371.090606	224740.293497	38.569344
2373.539483	224991.994363	38.574362
2375.746414	225249.029361	38.579380
2378.414400	225482.780379	38.584397
2380.713793	225721.542679	38.589415
2382.552566	225964.302354	38.594432
2384.671287	226209.189719	38.599450
2386.738102	226461.628657	38.604468
2389.197510	226715.301328	38.609485
2391.206491	226976.842797	38.614503
2393.742797	227235.838050	38.619520
2395.935077	227497.504451	38.624538
2398.279523	227771.464801	38.629556
2400.608632	228040.019002	38.634573
2402.835654	228322.253585	38.639591
2405.442597	228592.543224	38.644608
2407.723637	228884.193232	38.649626
2410.262734	229160.057267	38.654644
2412.593988	229453.783741	38.659661
2414.841847	229748.464093	38.664679
2417.368936	230033.374075	38.669696
2419.784850	230327.623337	38.674714
2422.229541	230624.535704	38.679732
2424.539966	230925.813261	38.684749
2427.136819	231227.046407	38.689767
2429.849832	231517.798358	38.694784
2432.121812	231827.593105	38.699802
2434.599803	232121.863654	38.704820
2437.436232	232416.281492	38.709837
2439.662223	232724.791187	38.714855
2442.271089	233013.913398	38.719872
2444.534243	233328.057470	38.724890
2446.865867	233622.812995	38.729908
2449.603552	233928.019873	38.734925
2452.082446	234233.929067	38.739943
2454.790827	234542.495050	38.744960
2457.256214	234849.043231	38.749978
2459.666396	235150.013437	38.754996
2462.870392	235459.722807	38.760013
2464.896900	235773.302525	38.765031
2467.345193	236061.087505	38.770048
2469.817835	236380.744832	38.775066
2472.359710	236676.136299	38.780084
2474.989388	236975.959481	38.785101
2477.164765	237280.986095	38.790119
2479.857105	237583.442542	38.795136
2482.576422	237895.699612	38.800154
2484.913207	238199.941265	38.805172
2487.647788	238496.729541	38.810189
2490.284909	238805.116140	38.815207
2492.853728	239104.650034	38.820224
2495.328095	239414.334069	38.825242
2498.136645	239708.065898	38.830260
2500.777354	240005.101624	38.835277
2503.122582	240302.057940	38.840295
2505.568721	240586.730968	38.845312
2507.884947	240869.672690	38.850330
2510.393938	241142.958010	38.855348
2512.643867	241405.921862	38.860365
2514.740745	241679.705511	38.865383
2517.211728	241944.565900	38.870400
2519.494002	242218.676982	38.875418
2521.883735	242504.328690	38.880436
2524.368157	242794.639678	38.885453
2526.658979	243080.359177	38.890471
2529.237457	243360.750483	38.895488
2531.772100	243655.779940	38.900506
2534.008863	243951.136678	38.905524
2536.723071	244249.771291	38.910541
2538.710244	244569.172395	38.915559
2541.310635	244874.836996	38.920576
2543.755785	245181.492116	38.925594
2545.876203	245505.370244	38.930612
2548.718007	245824.130887	38.935629
2551.485521	246150.575077	38.940647
2553.982381	246470.407889	38.945664
2556.199099	246799.861957	38.950682
2558.740026	247122.432551	38.955700
2561.912089	247454.276840	38.960717
2564.412723	247789.327201	38.965735
2567.040095	248119.278009	38.970752
2569.629991	248448.600450	38.975770
2571.900668	248789.836567	38.980788
2574.996539	249118.877073	38.985805
2577.527620	249459.438374	38.990823
2580.255653	249792.907610	38.995840
2582.914351	250131.519624	39.000858
2585.586251	250459.588622	39.005876
2588.355486	250790.894255	39.010893
2590.826756	251138.733408	39.015911
2593.479859	251474.910502	39.020928
2596.078271	251811.528750	39.025946
2598.746945	252154.283746	39.030964
2601.519814	252484.271188	39.035981
2603.961644	252826.479179	39.040999
2606.855721	253149.894957	39.046016
2609.773240	253482.274479	39.051034
2611.796895	253830.697857	39.056052
2615.000176	254155.996941	39.061069
2617.384436	254508.936791	39.066087
2620.111297	254835.480984	39.071104
2623.042128	255178.784236	39.076122
2625.548522	255517.582912	39.081140
2628.558195	255851.653799	39.086157
2630.953868	256183.942719	39.091175
2633.701587	256513.712359	39.096192
2636.481405	256843.706035	39.101210
2638.985846	257181.491564	39.106228
2641.877527	257509.741141	39.111245
2644.414964	257835.837290	39.116263
2647.088459	258164.706617	39.121280
2649.761570	258476.734566	39.126298
2652.109661	258791.684895	39.131316
2654.665012	259092.199511	39.136333
2657.209845	259396.221716	39.141351
2659.784650	259694.930375	39.146368
2661.894521	259992.138057	39.151386
2664.162711	260316.552719	39.156404
2667.090999	260620.845827	39.161421
2669.195360	260955.981755	39.166439
2671.522132	261272.513385	39.171456
2674.335954	261611.652951	39.176474
2676.952587	261946.327829	39.181492
2679.430224	262280.288405	39.186509
2681.899091	262640.745982	39.191527
2684.881186	262994.848135	39.196544
2687.343287	263340.700853	39.201562
2689.866830	263700.490441	39.206580
2692.660685	264047.358241	39.211597
2695.418782	264412.217402	39.216615
2698.161589	264782.820435	39.221632
2701.069847	265134.904154	39.226650
2703.678388	265510.203308	39.231668
2706.704332	265879.339929	39.236685
2709.055505	266236.898282	39.241703
2711.812179	266608.212026	39.246720
2714.974044	266983.780433	39.251738
2717.501749	267358.128600	39.256756
2720.314899	267727.986261	39.261773
2723.163872	268098.092533	39.266791
2726.115814	268475.575092	39.271808
2728.980437	268851.572924	39.276826
2731.615392	269217.141190	39.281844
2734.294342	269593.092645	39.286861
2737.466079	269975.825151	39.291879
2739.977022	270341.845486	39.296896
2743.273279	270715.083177	39.301914
2745.507213	271099.895383	39.306932
2748.785128	271459.215233	39.311949
2751.653513	271835.925171	39.316967
2754.333227	272202.605365	39.321984
2757.406408	272577.098401	39.327002
2759.851240	272950.649501	39.332020
2762.848170	273321.344273	39.337037
2765.943894	273692.658551	39.342055
2768.973983	274054.634821	39.347072
2772.030370	274397.528998	39.352090
2774.585767	274776.727816	39.357108
2777.715999	275139.374202	39.362125
2780.520191	275488.532203	39.367143
2782.938109	275851.596231	39.372160
2785.572649	276212.619065	39.377178
2788.355185	276577.327332	39.382196
2791.166715	276935.756322	39.387213
2793.955839	277301.936846	39.392231
2796.330165	277670.723329	39.397248
2799.341704	278031.228933	39.402266
2801.940450	278364.999242	39.407284
2804.481792	278699.439045	39.412301
2807.294138	279037.138278	39.417319
2809.704071	279371.141430	39.422336
2812.613909	279710.298402	39.427354
2814.665257	280066.890868	39.432372
2817.539966	280425.639106	39.437389
2820.301852	280788.266353	39.442407
2822.732952	281155.061135	39.447424
2825.604335	281507.229918	39.452442
2828.113114	281892.353176	39.457460
2830.801177	282273.891347	39.462477
2833.678940	282651.106082	39.467495
2836.168840	283041.286814	39.472512
2838.747065	283434.222218	39.477530
2841.633783	283840.724575	39.482548
2844.606660	284239.515784	39.487565
2847.803898	284640.379579	39.492583
2850.384790	285040.908740	39.497600
2853.632564	285454.973388	39.502618
2856.273562	285862.935331	39.507636
2858.925392	286273.359220	39.512653
2861.960446	286687.532430	39.517671
2864.692081	287099.974991	39.522688
2868.011522	287519.995681	39.527706
2870.917595	287954.560949	39.532724
2873.765138	288366.424723	39.537741
2876.558306	288785.612579	39.542759
2879.683168	289218.439451	39.547776
2882.976602	289632.110708	39.552794
2885.469579	290067.983064	39.557812
2888.761253	290484.549249	39.562829
2891.708239	290905.462405	39.567847
2894.359896	291344.228865	39.572864
2897.399535	291769.037940	39.577882
2900.414845	292207.643703	39.582900
2903.391880	292626.669420	39.587917
2905.930247	293068.321190	39.592935
2908.808918	293500.011307	39.597952
2912.008214	293932.792937	39.602970
2914.739257	294370.347258	39.607988
2917.573190	294809.357722	39.613005
2920.954436	295252.497379	39.618023
2923.666710	295689.340643	39.623040
2926.594943	296119.239404	39.628058
2929.649963	296570.175405	39.633076
2932.459155	297003.952146	39.638093
2935.465705	297448.340029	39.643111
2938.326911	297893.740516	39.648128
2941.110323	298333.665438	39.653146
2944.205416	298787.714067	39.658164
2947.433566	299243.315345	39.663181
2950.457440	299680.175992	39.668199
2953.264324	300120.041817	39.673216
2955.861770	300562.733770	39.678234
2958.767169	300981.371488	39.683252
2961.444400	301392.347628	39.688269
2964.411656	301795.173791	39.693287
2966.783046	302226.618703	39.698304
2970.146112	302637.254343	39.703322
2972.856167	303070.319693	39.708340
2975.310636	303503.373418	39.713357
2978.330034	303929.859208	39.718375
2981.310747	304369.939254	39.723392
2984.043508	304814.730890	39.728410
2986.690931	305267.307184	39.733428
2989.661310	305716.452584	39.738445
2992.911258	306175.280593	39.743463
2995.529055	306631.032017	39.748480
2998.669229	307090.915606	39.753498
3001.609535	307556.595013	39.758516
3004.232873	308039.340911	39.763533
3007.633739	308509.566693	39.768551
3010.534745	308997.497290	39.773568
3013.495883	309484.705207	39.778586
3016.528156	309968.318521	39.783604
3020.067855	310466.327277	39.788621
3023.080764	310946.917051	39.793639
3026.016531	311444.178973	39.798656
3029.203254	311926.870631	39.803674
3032.256216	312410.444932	39.808692
3034.971207	312912.713450	39.813709
3038.483912	313411.653134	39.818727
3041.570666	313909.591151	39.823744
3044.705761	314399.620191	39.828762
3047.708676	314913.821829	39.833780
3051.027403	315400.540661	39.838797
3054.086978	315901.876776	39.843815
3056.717089	316412.447073	39.848832
3060.409490	316902.833005	39.853850
3063.635218	317413.684824	39.858868
3066.288811	317919.722720	39.863885
3069.935276	318412.394063	39.868903
3072.955391	318910.876385	39.873920
3076.338774	319422.962326	39.878938
3079.450132	319915.786607	39.883956
3082.413813	320416.072933	39.888973
3085.828635	320908.513641	39.893991
3088.879726	321418.990104	39.899008
3092.227113	321920.400930	39.904026
3095.231567	322410.815675	39.909044
3098.241223	322908.515562	39.914061
3101.497880	323397.208616	39.919079
3104.536896	323892.688634	39.924096
3107.763668	324386.129738	39.929114
3110.973652	324885.056043	39.934132
3114.106309	325377.668053	39.939149
3117.323836	325876.079203	39.944167
3120.548852	326374.562268	39.949184
3123.750693	326851.815573	39.954202
3126.629290	327301.284258	39.959220
3129.162337	327764.264293	39.964237
3132.517370	328211.798525	39.969255
3135.366105	328665.403369	39.974272
3138.344021	329126.070107	39.979290
3141.400368	329588.499225	39.984308
3143.907804	330059.366982	39.989325
3147.096398	330533.120467	39.994343
3149.682739	331024.564041	39.999360
3152.840739	331505.984989	40.004378
3155.742442	331998.032326	40.009396
3158.696575	332510.534915	40.014413
3161.630202	333014.047931	40.019431
3164.521351	333536.837232	40.024448
3167.948137	334047.806483	40.029466
3170.991492	334570.563941	40.034484
3173.960519	335103.740003	40.039501
3177.084256	335636.125652	40.044519
3180.506702	336168.002792	40.049536
3183.631958	336710.891909	40.054554
3186.968003	337256.561683	40.059572
3189.934757	337801.929871	40.064589
3193.706114	338344.957189	40.069607
3196.590201	338895.915278	40.074624
3200.396903	339441.568386	40.079642
3203.587892	340003.030833	40.084660
3206.680949	340545.994363	40.089677
3210.139640	341097.020098	40.094695
3213.341676	341643.384437	40.099712
3216.805370	342198.411101	40.104730
3220.537470	342741.863541	40.109748
3223.508717	343298.608328	40.114765
3226.940176	343839.483339	40.119783
3230.487863	344395.923588	40.124800
3233.549922	344929.103574	40.129818
3237.140128	345491.112136	40.134836
3239.908364	346040.805254	40.139853
3243.617629	346577.193517	40.144871
3246.526545	347139.420688	40.149888
3250.157039	347696.222250	40.154906
3253.525336	348239.071641	40.159924
3256.902671	348790.977324	40.164941
3260.778373	349334.091177	40.169959
3263.687157	349878.291887	40.174976
3267.399433	350409.921039	40.179994
3270.786388	350960.381742	40.185012
3273.817543	351491.016403	40.190029
3277.212571	352037.047732	40.195047
3280.499201	352579.105175	40.200064
3283.660110	353117.039248	40.205082
3287.252488	353649.670389	40.210100
3290.117232	354188.046399	40.215117
3293.505346	354728.263180	40.220135
3296.503335	355285.492115	40.225152
3300.090498	355803.963179	40.230170
3303.410771	356315.440063	40.235188
3306.455653	356812.664844	40.240205
3309.751244	357309.641964	40.245223
3312.513620	357811.647959	40.250240
3315.741542	358308.346545	40.255258
3318.962659	358808.569224	40.260276
3321.785776	359328.190331	40.265293
3324.893240	359851.923397	40.270311
3327.919841	360380.155958	40.275328
3331.049539	360905.625283	40.280346
3334.272197	361458.154837	40.285364
3337.471924	362011.620612	40.290381
3340.578767	362565.170688	40.295399
3343.934674	363124.207503	40.300416
3347.043787	363695.306267	40.305434
3350.759971	364254.272428	40.310452
3353.905438	364836.543255	40.315469
3357.223905	365417.028177	40.320487
3360.483185	365992.414065	40.325504
3363.801757	366578.035678	40.330522
3367.564763	367159.214459	40.335540
3370.579325	367749.385827	40.340557
3374.430128	368346.826958	40.345575
3377.806529	368934.032260	40.350592
3381.156505	369529.354033	40.355610
3385.081451	370136.909105	40.360628
3387.996373	370734.110028	40.365645
3391.964560	371340.600784	40.370663
3395.007611	371928.756658	40.375680
3398.611141	372539.220868	40.380698
3402.175428	373134.483616	40.385716
3405.671808	373749.793395	40.390733
3409.266740	374344.830926	40.395751
3412.825305	374942.935650	40.400768
3416.320990	375549.693425	40.405786
3419.980789	376143.121413	40.410804
3423.522196	376752.594055	40.415821
3426.807336	377348.042455	40.420839
3430.479954	377945.780156	40.425856
3433.904792	378560.013245	40.430874
3437.743209	379143.321728	40.435892
3441.147539	379751.196982	40.440909
3444.791083	380335.761556	40.445927
3448.270060	380932.088987	40.450944
3451.777721	381537.306886	40.455962
3455.271353	382130.594560	40.460980
3458.499207	382733.605355	40.465997
3462.179852	383328.138477	40.471015
3465.798043	383923.737476	40.476032
3469.128499	384526.449654	40.481050
3472.887925	385116.578919	40.486068
3476.588616	385720.380004	40.491085
3479.739927	386311.245803	40.496103
3483.304422	386897.750137	40.501120
3486.833229	387481.012877	40.506125
3489.899394	388022.620379	40.511130
3492.964548	388514.151613	40.516135
3495.896188	388952.629046	40.521140
3498.490408	389356.191365	40.526144
3500.751487	389705.081937	40.531149
3503.537112	389986.580290	40.536154
3505.164975	390242.196686	40.541159
3506.911581	390437.784965	40.546164
3508.544377	390598.936838	40.551168
3509.676728	390732.350267	40.556173
3511.422052	390827.144945	40.561178
3512.499420	390879.251999	40.566183
3513.192277	390907.722185	40.571188
3514.387140	390915.568321	40.576192
3514.991498	390906.548268	40.581197
3515.635351	390857.246221	40.586202
3515.924193	390801.414717	40.591207
3516.219079	390729.487062	40.596212
3516.630740	390628.249152	40.601216
3516.818823	390540.242832	40.606221
3517.381945	390418.333769	40.611226
3517.478192	390302.295447	40.616231
3517.565680	390155.999860	40.621236
3517.469791	390030.786398	40.626240
3517.151598	389887.223686	40.631245
3517.422214	389729.683942	40.636250
3517.250363	389596.547596	40.641255
3517.017705	389429.372759	40.646260
3517.046611	389267.114205	40.651264
3516.449827	389114.158711	40.656269
3516.417846	388957.095659	40.661274
3516.484992	388802.508202	40.666279
3516.032991	388649.095555	40.671284
3515.809182	388495.646181	40.676288
3515.486150	388349.331793	40.681293
3515.730209	388196.697179	40.686298
3514.694494	388045.154221	40.691303
3514.658071	387881.577441	40.696308
3515.077650	387745.619857	40.701312
3514.427586	387595.819499	40.706317
3514.145174	387461.777271	40.711322
3513.657763	387337.430022	40.716327
3513.634239	387189.639563	40.721332
3513.679797	387062.715060	40.726336
3512.762762	386933.882495	40.731341
3513.228999	386809.230115	40.736346
3512.744949	386680.429928	40.741351
3512.552986	386562.645021	40.746356
3512.395177	386426.544911	40.751360
3512.059687	386323.098875	40.756365
3512.044630	386200.961768	40.761370
3511.364610	386093.424468	40.766375
3511.371315	385982.472389	40.771380
3511.303474	385867.768097	40.776384
3510.698442	385779.722945	40.781389
3511.306186	385673.430373	40.786394
3510.659353	385571.760696	40.791399
3510.619653	385484.439244	40.796404
3510.189465	385388.227784	40.801408
3510.050903	385284.162795	40.806413
3509.736357	385210.184317	40.811418
3509.253241	385130.459580	40.816423
3509.467353	385055.990335	40.821428
3509.835441	384969.010096	40.826432
3509.140208	384901.576025	40.831437
3509.238786	384810.391071	40.836442
3509.371284	384736.569859	40.841447
3508.976796	384662.602926	40.846452
3508.920194	384607.833718	40.851456
3508.642261	384537.052418	40.856461
3508.578384	384449.147435	40.861466
3508.326458	384399.520452	40.866471
3508.193848	384321.137284	40.871476
3508.335203	384264.174625	40.876480
3507.940884	384213.298341	40.881485
3508.280177	384144.707543	40.886490
3507.770802	384097.842008	40.891495
3507.643587	384032.732551	40.896500
3507.382695	383987.862111	40.901504
3507.386096	383931.124204	40.906509
3507.182328	383880.446228	40.911514
3507.013774	383828.770787	40.916519
3507.033723	383779.761224	40.921524
3507.057435	383750.282475	40.926528
3506.946923	383711.593242	40.931533
3507.142643	383647.322174	40.936538
3506.980622	383607.827163	40.941543
3506.958433	383587.968723	40.946548
3506.950481	383533.291977	40.951552
3506.701788	383497.065814	40.956557
3506.929547	383453.007601	40.961562
3506.678756	383416.807124	40.966567
3506.421195	383369.417667	40.971572
3506.405082	383324.584036	40.976576
3506.277649	383308.378844	40.981581
3506.706340	383262.661004	40.986586
3506.097221	383233.205592	40.991591
3506.070810	383192.620566	40.996596
3506.193197	383157.454423	41.001600
3506.444243	383131.728621	41.006605
3506.415671	383100.095907	41.011610
3505.950304	383069.829249	41.016615
3505.995761	383035.158362	41.021620
3506.295173	383006.169523	41.026624
3505.924662	382984.204098	41.031629
3506.094471	382941.527782	41.036634
3505.980802	382917.716035	41.041639
3505.934581	382885.068644	41.046644
3506.050009	382859.186070	41.051648
3505.921126	382830.671715	41.056653
3506.013786	382791.974853	41.061658
3505.656635	382779.417127	41.066663
3505.484205	382746.865864	41.071668
3506.041048	382717.658084	41.076672
3505.556139	382701.865193	41.081677
3505.834351	382662.731950	41.086682
3505.873970	382642.583487	41.091687
3505.631248	382611.823484	41.096692
3505.697403	382590.577206	41.101696
3505.249437	382564.859788	41.106701
3505.719259	382548.280101	41.111706
3505.603368	382522.789917	41.116711
3505.321499	382503.404308	41.121716
3505.822948	382477.384154	41.126720
3505.421985	382466.867846	41.131725
3505.519501	382432.798558	41.136730
3505.295612	382418.922589	41.141735
3505.058684	382395.155431	41.146740
3505.083407	382372.974577	41.151744
3504.751771	382357.716830	41.156749
3505.351053	382336.742189	41.161754
3505.450115	382322.408212	41.166759
3505.210716	382306.169426	41.171764
3505.373612	382273.335856	41.176768
3505.266248	382270.250263	41.181773
3505.212698	382244.292251	41.186778
3505.431938	382220.707199	41.191783
3504.884010	382198.845662	41.196788
3505.028623	382187.403755	41.201792
3504.797247	382172.257247	41.206797
3505.028353	382159.708054	41.211802
3504.990099	382151.575858	41.216807
3504.639311	382136.321049	41.221812
3505.404886	382115.701490	41.226816
3505.060961	382109.601356	41.231821
3504.923948	382091.515138	41.236826
3504.810664	382074.060978	41.241831
3505.089363	382059.418746	41.246836
3505.461862	382041.429990	41.251840
3504.781635	382031.415496	41.256845
3505.222995	382014.433153	41.261850
3505.197744	381984.706440	41.266855
3505.201879	381982.366182	41.271860
3505.212668	381952.913509	41.276864
3504.973846	381925.077106	41.281869
3505.125293	381915.897559	41.286874
3505.006301	381900.784043	41.291879
3504.827781	381896.387161	41.296884
3504.837716	381870.749486	41.301888
3504.636306	381870.756104	41.306893
3505.065119	381835.565730	41.311898
3504.792622	381839.830877	41.316903
3504.639301	381822.484663	41.321908
3504.827353	381810.196491	41.326912
3505.138692	381795.930491	41.331917
3504.744153	381787.040686	41.336922
3504.871684	381758.586725	41.341927
3504.733108	381762.423783	41.346932
3505.069260	381729.486058	41.351936
3504.646923	381730.544918	41.356941
3504.937014	381706.210792	41.361946
3505.047338	381700.674609	41.366951
3504.933779	381681.745201	41.371956
3504.860813	381677.636803	41.376960
3504.681956	381661.133841	41.381965
3504.790135	381658.217590	41.386970
3504.800426	381628.256085	41.391975
3504.813422	381625.736373	41.396980
3504.725941	381613.974922	41.401984
3504.867115	381597.650239	41.406989
3505.013353	381574.915619	41.411994
3505.022705	381558.993255	41.416999
3504.648300	381547.353439	41.422004
3504.768666	381529.124535	41.427008
3504.827521	381511.998971	41.432013
3504.972030	381501.345301	41.437018
3504.861766	381495.716793	41.442023
3505.013672	381478.271307	41.447028
3504.899838	381445.251872	41.452032
3504.537851	381466.520544	41.457037
3504.617853	381431.232340	41.462042
3504.933339	381429.605825	41.467047
3504.934922	381418.516929	41.472052
3504.783240	381406.256900	41.477056
3504.724161	381383.630922	41.482061
3504.509913	381357.672277	41.487066
3504.480971	381358.770692	41.492071
3504.628965	381340.944263	41.497076
3504.649731	381333.590993	41.502080
3504.590018	381327.064307	41.507085
3504.607587	381310.046911	41.512090
3504.708928	381299.196544	41.517095
3504.809259	381290.508159	41.522100
3504.675793	381282.187363	41.527104
3504.620179	381256.203573	41.532109
3504.854823	381242.076658	41.537114
3504.228485	381240.624451	41.542119
3504.150342	381239.314486	41.547124
3504.568452	381227.905358	41.552128
3504.372480	381232.921473	41.557133
3504.872879	381218.574506	41.562138
3504.729407	381215.952336	41.567143
3504.679710	381192.358297	41.572148
3504.823822	381177.889603	41.577152
3504.682271	381167.942328	41.582157
3504.561000	381149.344509	41.587162
3504.541141	381142.989525	41.592167
3504.409451	381123.147106	41.597172
3504.582917	381119.711827	41.602176
3504.517513	381106.039227	41.607181
3504.213501	381098.762686	41.612186
3504.491692	381104.441431	41.617191
3504.060277	381087.087978	41.622196
3504.111847	381077.847719	41.627200
3504.603522	381075.455769	41.632205
3504.544051	381070.455004	41.637210
3504.664891	381054.031571	41.642215
3504.685254	381053.596196	41.647220
3504.637709	381045.032866	41.652224
3504.517644	381028.393171	41.657229
3504.689136	381017.226433	41.662234
3504.798613	381004.772391	41.667239
3504.503784	380986.736031	41.672244
3504.964535	380974.429917	41.677248
3504.767608	380980.260087	41.682253
3504.642744	380945.029256	41.687258
3504.889271	380935.605543	41.692263
3504.629585	380929.924272	41.697268
3504.830402	380909.647679	41.702272
3504.790712	380899.277296	41.707277
3504.794014	380890.629593	41.712282
3504.866861	380869.966272	41.717287
3504.465965	380857.465694	41.722292
3504.587691	380843.483651	41.727296
3504.201163	380828.768074	41.732301
3504.556191	380810.120231	41.737306
3504.598272	380819.040971	41.742311
3504.466660	380806.650410	41.747316
3504.825647	380792.096737	41.752320
3504.358292	380787.567351	41.757325
3504.438983	380763.850703	41.762330
3504.696634	380764.064522	41.767335
3504.495433	380756.186691	41.772340
3504.618052	380740.220648	41.777344
3504.709871	380738.120789	41.782349
3504.474048	380710.791703	41.787354
3504.263940	380711.995076	41.792359
3504.299043	380698.687948	41.797364
3504.624868	380678.238870	41.802368
3504.501671	380677.699017	41.807373
3504.697009	380660.678667	41.812378
3504.721955	380650.145397	41.817383
3504.544604	380638.931961	41.822388
3504.595908	380623.155179	41.827392
3503.935475	380632.365052	41.832397
3504.404329	380611.562691	41.837402
3504.370719	380600.809761	41.842407
3504.206860	380592.493620	41.847412
3504.574463	380589.485411	41.852416
3504.578662	380581.371605	41.857421
3504.554924	380565.123422	41.862426
3504.488986	380561.090094	41.867431
3504.343974	380550.710833	41.872436
3504.493341	380540.895444	41.877440
3504.319936	380536.319560	41.882445
3504.361794	380505.207672	41.887450
3504.233554	380510.416644	41.892455
3504.380906	380513.114975	41.897460
3504.379229	380485.519812	41.902464
3504.134845	380493.239657	41.907469
3504.297166	380480.827959	41.912474
3504.544185	380478.856155	41.917479
3504.352619	380479.090120	41.922484
3504.290032	380461.779816	41.927488
3503.987429	380449.848544	41.932493
3504.117115	380432.635001	41.937498
3504.598121	380435.051690	41.942503
3504.325456	380449.668576	41.947508
3504.563617	380428.317607	41.952512
3504.376200	380415.325330	41.957517
3504.235930	380412.270223	41.962522
3504.609401	380401.630923	41.967527
3504.259819	380385.815682	41.972532
3504.612819	380379.070990	41.977536
3504.307905	380372.532035	41.982541
3504.476813	380358.338887	41.987546
3504.710963	380352.528598	41.992551
3504.218268	380343.501370	41.997556
3504.467195	380330.440087	42.002560
3504.297138	380332.145818	42.007565
3504.439235	380320.729187	42.012570
3504.604389	380298.346899	42.017575
3504.374467	380298.663230	42.022580
3504.457831	380273.419825	42.027584
3504.037859	380272.163862	42.032589
3504.191580	380276.565276	42.037594
3504.352423	380272.699540	42.042599
3504.270275	380266.735767	42.047604
3504.678149	380247.494320	42.052608
3504.678769	380235.972860	42.057613
3504.742718	380216.175350	42.062618
3504.585588	380223.525380	42.067623
3504.243592	380196.848563	42.072628
3504.992612	380174.806283	42.077632
3504.421400	380176.880643	42.082637
3504.473812	380153.117224	42.087642
3504.559546	380142.574207	42.092647
3504.115878	380131.173816	42.097652
3504.422816	380123.571606	42.102656
3504.615776	380118.352775	42.107661
3504.420186	380104.496928	42.112666
3504.218711	380098.297652	42.117671
3504.147680	380090.628014	42.122676
3504.436419	380075.907139	42.127680
3504.141290	380067.789675	42.132685
3504.291039	380058.024971	42.137690
3504.413447	380063.194381	42.142695
3504.373794	380055.290869	42.147700
3504.441591	380041.647705	42.152704
3504.419888	380037.454726	42.157709
3504.313339	380016.107154	42.162714
3504.462917	380016.694139	42.167719
3504.496560	380005.599770	42.172724
3504.407552	379989.844911	42.177728
3504.282367	379974.655315	42.182733
3504.385206	379976.673999	42.187738
3504.468761	379956.186537	42.192743
3504.002305	379952.191026	42.197748
3504.350579	379947.558039	42.202752
3504.236895	379946.482555	42.207757
3504.340707	379934.410576	42.212762
3504.466170	379916.027501	42.217767
3504.128432	379922.007260	42.222772
3504.639375	379909.972651	42.227776
3504.269023	379907.335387	42.232781
3504.197065	379882.777570	42.237786
3504.378354	379883.257808	42.242791
3504.432153	379877.577694	42.247796
3504.176377	379860.297660	42.252800
3504.134286	379869.333662	42.257805
3504.232276	379849.683190	42.262810
3504.418147	379830.603802	42.267815
3503.966372	379837.797008	42.272820
3504.306553	379826.501525	42.277824
3504.310705	379820.981857	42.282829
3503.926907	379807.181090	42.287834
3504.108917	379797.106011	42.292839
3503.931255	379807.180827	42.297844
3504.325442	379812.459913	42.302848
3504.202209	379793.683712	42.307853
3503.913904	379780.274789	42.312858
3504.286995	379791.025573	42.317863
3503.883051	379795.133684	42.322868
3504.023364	379771.279833	42.327872
3504.012577	379762.532369	42.332877
3503.942037	379756.642985	42.337882
3504.247577	379761.249366	42.342887
3504.242888	379755.247835	42.347892
3504.124641	379750.993784	42.352896
3504.071903	379732.638792	42.357901
3504.289545	379717.776416	42.362906
3504.202061	379735.034897	42.367911
3503.937771	379728.133332	42.372916
3504.261382	379716.713265	42.377920
3504.219113	379699.526580	42.382925
3504.373251	379707.081844	42.387930
3504.593324	379692.320811	42.392935
3504.386678	379690.802198	42.397940
3504.553350	379671.166213	42.402944
3504.246604	379661.727916	42.407949
3504.417470	379642.676243	42.412954
3504.535811	379638.868032	42.417959
3504.377483	379630.372770	42.422964
3504.344307	379613.286347	42.427968
3504.176295	379609.370794	42.432973
3503.946902	379604.473004	42.437978
3503.905003	379583.572793	42.442983
3504.033917	379583.298283	42.447988
3503.860671	379577.221633	42.452992
3503.911525	379580.418537	42.457997
3504.300356	379587.504340	42.463002
3503.972166	379586.589926	42.468007
3503.858583	379575.900223	42.473012
3504.004544	379557.996993	42.478016
3504.022587	379564.861636	42.483021
3504.191713	379562.952969	42.488026
3503.971566	379563.598407	42.493031
3504.044296	379558.881761	42.498036
3504.021532	379538.003935	42.503040
3503.906032	379534.003770	42.508045
3504.293523	379529.873223	42.513050
3504.284127	379535.419620	42.518055
3503.983547	379528.625494	42.523060
3503.974614	379518.962043	42.528064
3504.078879	379503.049262	42.533069
3503.632736	379513.064858	42.538074
3503.870268	379512.849480	42.543079
3503.660169	379519.088902	42.548084
3503.766351	379518.563640	42.553088
3503.597457	379521.032255	42.558093
3504.150344	379522.394828	42.563098
3504.362932	379502.573458	42.568103
3503.925899	379496.894577	42.573108
3504.390906	379494.532182	42.578112
3504.273569	379507.191851	42.583117
3504.448400	379481.501089	42.588122
3504.286009	379488.623178	42.593127
3504.223255	379484.182285	42.598132
3504.427839	379463.243046	42.603136
3504.114714	379460.316927	42.608141
3504.099099	379457.623555	42.613146
3504.032165	379453.208754	42.618151
3503.756956	379445.189748	42.623156
3503.946550	379430.560606	42.628160
3503.832824	379421.981945	42.633165
3503.709863	379424.239828	42.638170
3504.052562	379428.051906	42.643175
3503.716834	379422.789386	42.648180
3504.237420	379422.631000	42.653184
3503.961294	379414.739305	42.658189
3504.090396	379400.933619	42.663194
3504.338720	379394.459650	42.668199
3504.038325	379396.847321	42.673204
3503.976874	379401.155676	42.678208
3503.876001	379399.594896	42.683213
3504.036101	379375.407028	42.688218
3504.047391	379386.825546	42.693223
3503.888265	379381.433364	42.698228
3504.045934	379379.221285	42.703232
3503.687193	379386.120087	42.708237
3503.692536	379388.255952	42.713242
3504.095160	379375.704178	42.718247
3503.986788	379377.934323	42.723252
3504.136983	379359.292732	42.728256
3504.253319	379350.321603	42.733261
3504.136789	379358.606455	42.738266
3503.811412	379342.074794	42.743271
3504.047494	379332.703214	42.748276
3504.130884	379337.064983	42.753280
3503.830661	379338.562423	42.758285
3504.039854	379346.592311	42.763290
3504.215188	379320.138327	42.768295
3503.848566	379318.161731	42.773300
3503.963629	379313.641840	42.778304
3503.953652	379312.499075	42.783309
3504.026166	379307.477218	42.788314
3503.844107	379321.062822	42.793319
3503.829842	379311.908854	42.798324
3504.180901	379303.053216	42.803329
3504.229307	379293.558687	42.808333
3504.161759	379288.813315	42.813338
3504.357058	379281.940757	42.818343
3504.287730	379273.583955	42.823348
3504.190200	379263.171409	42.828353
3504.038179	379255.845059	42.833357
3504.247288	379260.848262	42.838362
3504.374849	379242.439104	42.843367
3504.125229	379232.864500	42.848372
3504.367596	379219.015409	42.853377
3504.297848	379217.602309	42.858381
3503.976663	379205.444681	42.863386
3504.360346	379190.683030	42.868391
3503.949022	379192.096299	42.873396
3504.077375	379187.625162	42.878401
3504.394975	379185.311486	42.883405
3504.252302	379161.298521	42.888410
3504.235465	379156.672289	42.893415
3503.716954	379164.690076	42.898420
3504.398572	379164.022976	42.903425
3504.303282	379136.339916	42.908429
3504.101160	379136.168603	42.913434
3503.865391	379124.531574	42.918439
3504.007390	379147.324230	42.923444
3504.178107	379121.557577	42.928449
3504.189589	379115.655131	42.933453
3504.157572	379106.275008	42.938458
3504.117204	379107.655074	42.943463
3503.850259	379105.408364	42.948468
3503.939924	379088.276858	42.953473
3504.104557	379082.451935	42.958477
3503.880436	379082.182360	42.963482
3504.126940	379076.573406	42.968487
3503.981896	379075.706332	42.973492
3504.378337	379063.689564	42.978497
3504.056692	379059.798242	42.983501
3504.207871	379050.389147	42.988506
3503.941127	379047.837185	42.993511
3503.815947	379060.396499	42.998516
3504.370069	379048.532843	43.003521
3504.234346	379036.066062	43.008525
3504.052505	379024.089828	43.013530
3504.113725	379019.781892	43.018535
3504.179383	379020.102376	43.023540
3503.916336	379001.856592	43.028545
3504.097519	379006.279243	43.033549
3504.039470	378990.926043	43.038554
3504.283216	378993.278590	43.043559
3503.708969	379003.746957	43.048564
3504.116960	378989.998778	43.053569
3504.156449	378975.723848	43.058573
3503.949905	378964.590847	43.063578
3504.047525	378970.730842	43.068583
3503.969924	378967.970931	43.073588
3504.404160	378954.829026	43.078593
3504.187425	378946.520891	43.083597
3504.244528	378939.619250	43.088602
3504.457166	378935.490847	43.093607
3503.821469	378919.847412	43.098612
3504.115679	378912.603066	43.103617
3504.235124	378907.751783	43.108621
3504.049512	378906.535031	43.113626
3504.038477	378900.686981	43.118631
3503.922625	378881.451349	43.123636
3504.151736	378864.348572	43.128641
3504.012716	378877.062741	43.133645
3504.010259	378880.293565	43.138650
3504.337509	378860.835268	43.143655
3504.003712	378852.647358	43.148660
3503.940747	378840.957494	43.153665
3503.935236	378836.202260	43.158669
3503.715598	378848.064398	43.163674
3504.010035	378835.427814	43.168679
3503.819555	378857.357541	43.173684
3504.085147	378841.749643	43.178689
3503.879752	378830.769031	43.183693
3503.541948	378824.870887	43.188698
3503.983253	378806.691711	43.193703
3503.799646	378820.099689	43.198708
3503.886031	378821.815816	43.203713
3503.641459	378831.087545	43.208717
3504.116607	378831.648517	43.213722
3503.904383	378817.769408	43.218727
3503.895400	378811.336018	43.223732
3504.338042	378801.855354	43.228737
3503.826440	378791.838793	43.233741
3503.986301	378800.181810	43.238746
3504.019560	378792.190212	43.243751
3503.650845	378795.911333	43.248756
3503.945322	378778.798186	43.253761
3503.643985	378773.784489	43.258765
3503.926073	378765.982465	43.263770
3503.707536	378767.975711	43.268775
3504.054820	378770.515384	43.273780
3504.193169	378768.560673	43.278785
3504.119147	378781.824167	43.283789
3503.720800	378754.748313	43.288794
3504.007447	378738.145084	43.293799
3503.661654	378743.719335	43.298804
3504.065028	378740.120329	43.303809
3504.335838	378751.930401	43.308813
3504.237140	378738.872669	43.313818
3504.040284	378731.985702	43.318823
3503.811258	378720.856187	43.323828
3503.931938	378721.702109	43.328833
3503.901533	378728.803472	43.333837
3503.751006	378725.520939	43.338842
3503.793822	378730.804847	43.343847
3503.443208	378734.853767	43.348852
3503.835215	378735.860277	43.353857
3504.190628	378725.452292	43.358861
3503.887065	378716.242177	43.363866
3504.079899	378706.165106	43.368871
3503.989464	378702.033719	43.373876
3504.244345	378696.347082	43.378881
3503.884849	378698.082830	43.383885
3503.684482	378684.532454	43.388890
3504.075133	378664.885993	43.393895
3504.130822	378679.680549	43.398900
3504.049014	378678.879775	43.403905
3503.995678	378682.245832	43.408909
3504.138154	378665.207533	43.413914
3504.377280	378643.651958	43.418919
3504.111984	378650.892207	43.423924
3504.139737	378644.936247	43.428929
3504.088393	378643.393042	43.433933
3503.800863	378641.429343	43.438938
3504.460362	378618.764467	43.443943
3503.911701	378618.851412	43.448948
3503.984739	378621.866843	43.453953
3504.144069	378626.598211	43.458957
3504.273030	378611.113560	43.463962
3504.128937	378587.990694	43.468967
3503.755541	378598.173067	43.473972
3504.094447	378591.328557	43.478977
3503.960715	378596.029951	43.483981
3503.862166	378595.994872	43.488986
3504.250763	378564.953800	43.493991
3503.928333	378564.776067	43.498996
3503.921199	378564.370446	43.504001
3503.820471	378567.006390	43.509005
3503.877744	378568.676260	43.514010
3503.882400	378556.085395	43.519015
3503.585885	378552.597010	43.524020
3503.899112	378539.245180	43.529025
3503.890729	378541.993703	43.534029
3503.697708	378540.650935	43.539034
3504.165744	378538.109960	43.544039
3503.992203	378546.989001	43.549044
3504.018046	378543.297047	43.554049
3503.947956	378543.664429	43.559053
3504.002205	378528.471342	43.564058
3504.228568	378511.114495	43.569063
3503.711356	378522.845726	43.574068
3503.494499	378512.833370	43.579073
3503.969239	378517.794677	43.584077
3503.671915	378525.625018	43.589082
3503.928427	378529.450809	43.594087
3503.605588	378518.539546	43.599092
3503.867962	378509.697751	43.604097
3503.784394	378504.624160	43.609101
3503.769743	378496.055069	43.614106
3504.227115	378488.225281	43.619111
3503.769102	378491.629891	43.624116
3503.797523	378488.446225	43.629121
3503.982476	378497.879048	43.634125
3504.056317	378481.385657	43.639130
3503.709383	378472.919958	43.644135
3504.091949	378464.262633	43.649140
3504.281096	378458.510048	43.654145
3504.205123	378450.128686	43.659149
3503.852515	378462.876754	43.664154
3504.022583	378458.907641	43.669159
3503.936571	378449.968295	43.674164
3503.766624	378443.941817	43.679169
3504.249716	378438.142762	43.684173
3504.123093	378430.812243	43.689178
3504.155637	378438.412409	43.694183
3504.165749	378417.554226	43.699188
3504.075258	378411.616923	43.704193
3504.062255	378409.380899	43.709197
3504.000197	378408.933089	43.714202
3504.239753	378397.449622	43.719207
3504.053622	378381.251636	43.724212
3504.063408	378368.456420	43.729217
3504.255768	378372.343237	43.734221
3504.084910	378377.788146	43.739226
3504.244188	378358.000063	43.744231
3503.993710	378337.742605	43.749236
3503.802331	378344.004688	43.754241
3504.372608	378331.629560	43.759245
3503.963523	378344.793556	43.764250
3503.781664	378308.246723	43.769255
3503.571522	378313.290888	43.774260
3503.835921	378305.796791	43.779265
3504.140830	378300.000448	43.784269
3503.952493	378297.868441	43.789274
3504.108008	378299.548227	43.794279
3503.582054	378311.280903	43.799284
3503.689189	378306.787585	43.804289
3503.612588	378316.388973	43.809293
3503.935219	378322.849592	43.814298
3504.135745	378297.332040	43.819303
3503.867217	378286.132341	43.824308
3503.734030	378285.594032	43.829313
3503.990004	378287.079892	43.834317
3504.156382	378278.609313	43.839322
3504.210264	378282.263678	43.844327
3503.937347	378275.821053	43.849332
3504.096265	378248.376971	43.854337
3504.119979	378250.433688	43.859341
3504.089476	378257.051882	43.864346
3504.341485	378243.099184	43.869351
3503.955105	378233.215297	43.874356
3503.928488	378223.223664	43.879361
3504.356114	378221.986256	43.884365
3504.256704	378223.884391	43.889370
3504.153794	378191.979620	43.894375
3503.705204	378196.247565	43.899380
3504.014860	378187.042129	43.904385
3503.842284	378193.199522	43.909389
3503.611714	378197.026038	43.914394
3504.178995	378193.604554	43.919399
3504.232874	378197.894809	43.924404
3503.940819	378179.449746	43.929409
3503.938547	378176.092861	43.934413
3503.738029	378169.079198	43.939418
3504.077663	378166.176968	43.944423
3503.805253	378180.413130	43.949428
3504.216033	378168.114036	43.954433
3504.117202	378145.797684	43.959437
3504.175366	378139.811406	43.964442
3504.408740	378135.170936	43.969447
3504.261551	378130.616060	43.974452
3504.074943	378113.248016	43.979457
3503.959099	378102.202174	43.984461
3503.957120	378100.295050	43.989466
3503.989177	378102.325020	43.994471
3503.797039	378107.213753	43.999476
3503.954059	378092.105993	44.004481
3504.072641	378080.361769	44.009485
3503.671516	378068.852309	44.014490
3504.192923	378069.965558	44.019495
3504.067674	378076.954854	44.024500
3504.040643	378072.635331	44.029505
3504.024031	378063.252525	44.034509
3504.325623	378048.605166	44.039514
3504.438859	378046.221989	44.044519
3503.972379	378051.103226	44.049524
3504.138760	378032.534754	44.054529
3503.799386	378011.985957	44.059533
3503.690676	378021.668800	44.064538
3504.039252	378003.325867	44.069543
3503.956211	378011.961802	44.074548
3503.771921	378010.007187	44.079553
3503.926425	378013.849154	44.084557
3503.948984	378004.409271	44.089562
3503.936322	377975.796660	44.094567
3503.663852	377988.862872	44.099572
3504.037569	377974.687356	44.104577
3503.905826	377978.269352	44.109581
3503.441435	377988.186476	44.114586
3503.534827	377974.869208	44.119591
3503.443816	377985.490371	44.124596
3503.748667	377990.504037	44.129601
3503.755817	377981.702470	44.134605
3504.035529	378000.836756	44.139610
3504.226223	377985.799938	44.144615
3503.556233	377971.662235	44.149620
3503.745738	377954.641631	44.154625
3503.928501	377965.499311	44.159629
3503.643786	377963.687746	44.164634
3503.548594	377971.181018	44.169639
3503.732526	377965.759846	44.174644
3503.641347	377970.327411	44.179649
3503.969225	377966.943752	44.184653
3504.184957	377969.478838	44.189658
3504.012777	377966.835550	44.194663
3503.927145	377952.274804	44.199668
3504.163735	377947.175966	44.204673
3504.172179	377933.261662	44.209677
3503.715289	377938.751847	44.214682
3504.082730	377939.762262	44.219687
3503.994093	377932.908918	44.224692
3503.994461	377918.614354	44.229697
3503.708484	377906.730548	44.234701
3503.438382	377897.286033	44.239706
3504.266435	377902.445921	44.244711
3504.028156	377915.430445	44.249716
3504.104652	377903.743693	44.254721
3504.353938	377900.855726	44.259725
3504.007730	377893.814174	44.264730
3504.083411	377878.948110	44.269735
3503.710903	377869.494341	44.274740
3503.912583	377868.089156	44.279745
3503.991617	377877.157339	44.284749
3503.898095	377871.398482	44.289754
3504.203846	377854.232282	44.294759
3503.708549	377854.209049	44.299764
3504.038069	377842.660329	44.304769
3503.839276	377839.970368	44.309773
3503.821059	377847.527802	44.314778
3504.046414	377844.312953	44.319783
3503.553890	377842.610539	44.324788
3503.440044	377828.537481	44.329793
3503.751476	377814.117400	44.334797
3503.352366	377831.095316	44.339802
3503.947541	377808.745372	44.344807
3503.689734	377810.948357	44.349812
3503.730105	377815.520580	44.354817
3503.784662	377817.521573	44.359821
3503.590661	377818.925970	44.364826
3503.839848	377818.708742	44.369831
3503.854523	377832.568985	44.374836
3503.824923	377835.295474	44.379841
3504.106415	377829.655378	44.384845
3503.721749	377836.100709	44.389850
3504.126333	377814.264171	44.394855
3503.571374	377809.392186	44.399860
3503.338844	377812.405112	44.404865
3503.685139	377793.731781	44.409869
3503.583595	377799.496474	44.414874
3503.611334	377805.545955	44.419879
3503.375927	377801.564568	44.424884
3503.706222	377791.363793	44.429889
3503.547372	377806.370639	44.434893
3503.799601	377800.913212	44.439898
3504.193380	377813.111095	44.444903
3503.818555	377810.321782	44.449908
3503.814058	377805.922361	44.454913
3503.992096	377815.737972	44.459917
3503.931109	377817.452005	44.464922
3504.252907	377792.372796	44.469927
3503.932023	377789.854746	44.474932
3504.075750	377784.796003	44.479937
3503.776114	377786.039051	44.484941
3503.899157	377790.242110	44.489946
3504.129263	377782.982257	44.494951
3504.049061	377771.549156	44.499956
3503.903485	377758.244156	44.504961
3504.210988	377759.238615	44.509965
3504.167633	377743.068669	44.514970
3503.764365	377749.313470	44.519975
3503.932603	377741.809033	44.524980
3504.062668	377722.126993	44.529985
3504.177582	377726.662006	44.534989
3503.882946	377724.114366	44.539994
3504.212771	377724.087875	44.544999
3504.155122	377705.605536	44.550004
3503.934291	377694.677920	44.555009
3503.944238	377689.207908	44.560013
3503.715717	377693.085019	44.565018
3503.866414	377683.141527	44.570023
3503.827581	377699.859062	44.575028
3503.939796	377701.545719	44.580033
3503.887852	377678.204269	44.585037
3503.368390	377678.210291	44.590042
3503.689593	377658.447133	44.595047
3503.955363	377658.964915	44.600052
3503.772483	377667.489530	44.605057
3503.912298	377668.357886	44.610061
3503.900212	377665.994498	44.615066
3503.987349	377657.739797	44.620071
3504.114289	377680.637423	44.625076
3503.703193	377662.160066	44.630081
3503.927417	377636.689215	44.635085
3503.769981	377639.461362	44.640090
3504.114980	377629.690627	44.645095
3503.830510	377641.385325	44.650100
3503.907651	377636.922108	44.655105
3503.761856	377642.871868	44.660109
3503.774429	377644.777764	44.665114
3504.099681	377630.864144	44.670119
3503.966904	377625.289507	44.675124
3503.972510	377618.828181	44.680129
3503.989529	377605.166764	44.685133
3503.918143	377614.436834	44.690138
3504.154575	377604.530641	44.695143
3503.975516	377605.373100	44.700148
3503.983164	377587.618018	44.705153
3503.989827	377582.708095	44.710157
3503.922723	377572.875313	44.715162
3503.898321	377568.987725	44.720167
3504.084720	377581.905225	44.725172
3503.863250	377578.252276	44.730177
3503.979472	377553.052801	44.735181
3503.760128	377556.903039	44.740186
3503.887744	377540.299012	44.745191
3503.842964	377557.195596	44.750196
3503.983753	377550.280483	44.755201
3503.884657	377543.505033	44.760205
3503.667690	377554.476886	44.765210
3504.127262	377526.908471	44.770215
3503.847635	377520.543091	44.775220
3503.747666	377505.628347	44.780225
3503.948990	377505.393248	44.785229
3503.749157	377510.588499	44.790234
3503.759148	377518.930042	44.795239
3504.052837	377508.684110	44.800244
3503.906294	377517.660856	44.805249
3503.969302	377521.364720	44.810253
3503.913641	377498.608773	44.815258
3504.045032	377486.379070	44.820263
3503.757138	377487.493093	44.825268
3503.870027	377487.526331	44.830273
3504.085252	377488.306463	44.835277
3503.722180	377489.788470	44.840282
3503.733940	377484.725115	44.845287
3504.225782	377473.862828	44.850292
3504.145325	377460.293076	44.855297
3504.177527	377450.749795	44.860301
3504.067347	377451.937468	44.865306
3504.220560	377426.197915	44.870311
3503.935668	377413.932253	44.875316
3504.041630	377426.353803	44.880321
3503.967925	377408.229965	44.885325
3503.725598	377418.519099	44.890330
3503.851418	377423.561139	44.895335
3503.870823	377421.421679	44.900340
3503.764569	377410.984588	44.905345
3504.019370	377400.999133	44.910349
3503.652592	377398.005033	44.915354
3503.909925	377384.814266	44.920359
3503.800716	377382.008369	44.925364
3503.706820	377386.907095	44.930369
3503.985185	377389.788418	44.935373
3503.687974	377379.788478	44.940378
3503.988748	377390.347867	44.945383
3504.041005	377383.217798	44.950388
3503.913449	377379.193883	44.955393
3503.917655	377366.653584	44.960397
3503.680600	377365.801017	44.965402
3504.007725	377366.080182	44.970407
3503.904878	377372.557345	44.975412
3504.019134	377372.412316	44.980417
3504.134465	377361.177110	44.985421
3503.769738	377351.289578	44.990426
3504.096192	377330.507995	44.995431
3503.821819	377341.412674	45.000436
3503.589284	377329.927220	45.005441
3503.762319	377337.861490	45.010445
3503.647553	377337.167642	45.015450
3503.934251	377332.467777	45.020455
3503.854686	377332.684054	45.025460
3503.730811	377331.915338	45.030465
3503.671988	377308.905424	45.035469
3503.552696	377304.346043	45.040474
3503.658799	377299.522109	45.045479
3503.645928	377304.026499	45.050484
3503.644066	377295.633178	45.055489
3503.867731	377300.023869	45.060493
3503.716846	377317.471481	45.065498
3503.758063	377306.883871	45.070503
3503.697378	377317.602162	45.075508
3503.670667	377315.953267	45.080513
3503.700085	377316.304931	45.085517
3503.736423	377308.694084	45.090522
3503.945752	377296.960719	45.095527
3503.839093	377315.520517	45.100532
3504.002103	377298.274899	45.105537
3504.340316	377280.492860	45.110541
3503.755437	377283.739576	45.115546
3504.032580	377278.379884	45.120551
3503.835867	377285.787590	45.125556
3504.016819	377289.294780	45.130561
3503.835250	377270.602906	45.135565
3503.843626	377256.790120	45.140570
3503.704020	377264.087059	45.145575
3503.880741	377258.234521	45.150580
3503.829263	377263.202865	45.155585
3504.192144	377257.244591	45.160589
3503.958178	377258.019429	45.165594
3503.828933	377255.292999	45.170599
3504.177373	377237.153222	45.175604
3504.019572	377230.386998	45.180609
3504.135319	377219.151686	45.185613
3503.875838	377220.108609	45.190618
3504.132113	377217.982566	45.195623
3503.902892	377203.367936	45.200628
3503.819933	377196.742491	45.205633
3504.087940	377171.162678	45.210637
3503.818718	377193.817978	45.215642
3503.695215	377195.007765	45.220647
3503.865520	377193.200542	45.225652
3503.860522	377198.390469	45.230657
3503.770462	377186.755271	45.235661
3503.745922	377196.323265	45.240666
3503.939544	377172.433981	45.245671
3503.713059	377169.443121	45.250676
3503.750459	377162.747773	45.255681
3503.953911	377156.763815	45.260685
3503.836126	377163.167065	45.265690
3503.974815	377162.585762	45.270695
3503.843889	377166.193137	45.275700
3503.733222	377164.964483	45.280705
3503.936056	377162.439910	45.285709
3503.676264	377146.838091	45.290714
3503.744473	377140.137868	45.295719
3503.813048	377139.822009	45.300724
3503.549105	377143.755644	45.305729
3503.672434	377131.756031	45.310733
3503.386767	377137.066642	45.315738
3503.643209	377134.686209	45.320743
3503.965307	377134.381144	45.325748
3503.679821	377136.893772	45.330753
3503.867068	377137.169615	45.335757
3503.708579	377140.908529	45.340762
3504.090917	377130.699359	45.345767
3503.719732	377154.566289	45.350772
3503.617958	377137.972922	45.355777
3503.896236	377122.693010	45.360781
3503.698210	377116.950564	45.365786
3503.997503	377108.306109	45.370791
3503.750009	377110.024218	45.375796
3503.599344	377105.062799	45.380801
3503.850833	377107.032697	45.385805
3503.747221	377103.946100	45.390810
3503.964050	377087.785630	45.395815
3503.804936	377093.101678	45.400820
3503.509945	377098.032229	45.405825
3503.998519	377087.704509	45.410829
3503.593297	377073.575502	45.415834
3503.667510	377055.885969	45.420839
3503.816057	377064.968784	45.425844
3503.867991	377062.111955	45.430849
3503.822608	377057.846095	45.435853
3503.876302	377059.262234	45.440858
3504.046130	377059.439088	45.445863
3503.708413	377053.413483	45.450868
3503.729688	377066.102893	45.455873
3504.111566	377057.852348	45.460877
3503.986237	377048.562797	45.465882
3503.703805	377025.003040	45.470887
3503.528719	377027.396480	45.475892
3503.849977	377025.209282	45.480897
3503.853196	377016.687919	45.485901
3503.690284	377028.389016	45.490906
3503.564253	377028.994179	45.495911
3503.767097	377027.715961	45.500916
3503.921358	377036.340031	45.505921
3504.253406	377006.451303	45.510925
3503.886669	377005.288560	45.515930
3503.766521	376995.718381	45.520935
3503.992775	376992.401578	45.525940
3504.100923	376988.264056	45.530945
3504.000236	376989.577423	45.535949
3503.765090	377005.385148	45.540954
3504.081263	376982.519255	45.545959
3503.609653	376975.624543	45.550964
3503.509081	376964.779460	45.555969
3503.716108	376959.685170	45.560973
3503.514551	376954.248492	45.565978
3503.526486	376960.275163	45.570983
3503.772082	376961.711842	45.575988
3503.499205	376967.198507	45.580993
3503.591401	376965.785161	45.585997
3503.655479	376974.805042	45.591002
3504.049007	376964.670368	45.596007
3503.891505	376967.544316	45.601012
3503.901042	376970.264678	45.606017
3504.123042	376974.655669	45.611021
3503.664669	376949.597518	45.616026
3503.501594	376938.838616	45.621031
3503.926420	376958.866162	45.626036
3503.636419	376965.067744	45.631041
3503.652749	376961.911304	45.636045
3503.566721	376968.767414	45.641050
3503.983225	376962.927800	45.646055
3504.074322	376973.901986	45.651060
3503.664104	376975.544081	45.656065
3504.141640	376967.431011	45.661069
3504.002277	376960.483775	45.666074
3503.900942	376948.901163	45.671079
3504.007006	376935.937649	45.676084
3503.772342	376927.046895	45.681089
3504.461058	376920.655522	45.686093
3503.660025	376940.444449	45.691098
3503.773579	376928.115650	45.696103
3504.017910	376929.577967	45.701108
3503.814990	376911.067353	45.706113
3503.998605	376902.339395	45.711117
3503.720348	376914.084196	45.716122
3503.673713	376904.146269	45.721127
3503.907296	376906.754910	45.726132
3503.608843	376917.561767	45.731137
3503.836721	376906.105152	45.736141
3503.433786	376916.267188	45.741146
3503.881361	376908.133407	45.746151
3503.943163	376916.187089	45.751156
3503.860689	376890.535320	45.756161
3503.809908	376871.110374	45.761165
3503.907395	376873.664222	45.766170
3503.737668	376867.306800	45.771175
3503.793531	376874.267677	45.776180
3503.706906	376874.459636	45.781185
3503.807103	376871.646036	45.786189
3503.561211	376872.829744	45.791194
3503.696767	376878.887758	45.796199
3503.884521	376880.918614	45.801204
3503.689841	376872.631993	45.806209
3503.994146	376863.961257	45.811213
3503.795688	376864.552437	45.816218
3503.874709	376841.469591	45.821223
3503.938358	376849.879100	45.826228
3503.871943	376839.003148	45.831233
3504.012653	376846.713700	45.836237
3503.750846	376846.780735	45.841242
3503.816278	376839.241508	45.846247
3504.128294	376815.104371	45.851252
3504.159333	376820.568448	45.856257
3504.246960	376807.785860	45.861261
3504.005618	376811.537902	45.866266
3504.175030	376802.252573	45.871271
3504.039430	376788.971109	45.876276
3503.721624	376793.778122	45.881281
3503.720975	376789.225364	45.886285
3503.984044	376790.048819	45.891290
3503.914215	376779.300571	45.896295
3503.956038	376789.239713	45.901300
3503.778740	376784.892932	45.906305
3503.825314	376756.727933	45.911309
3503.558797	376750.055123	45.916314
3503.717715	376753.514971	45.921319
3503.776335	376752.513905	45.926324
3503.717319	376753.133915	45.931329
3503.923084	376747.429329	45.936333
3503.736817	376757.302791	45.941338
3503.710062	376751.304293	45.946343
3503.676114	376763.773602	45.951348
3503.471411	376761.211683	45.956353
3503.883600	376761.909822	45.961357
3503.813544	376771.688601	45.966362
3504.014504	376770.741343	45.971367
3503.948401	376748.037492	45.976372
3503.606069	376733.237081	45.981377
3503.917264	376728.635019	45.986381
3503.624536	376733.921363	45.991386
3503.716602	376725.767437	45.996391
3503.871474	376725.895783	46.001396
3503.889865	376736.016697	46.006401
3503.871686	376730.271201	46.011405
3503.655053	376725.599961	46.016410
3503.688305	376725.187937	46.021415
3503.805481	376733.232903	46.026420
3503.759098	376716.605168	46.031425
3503.560500	376702.901218	46.036429
3503.509063	376700.238758	46.041434
3503.510200	376701.179931	46.046439
3503.810713	376703.930621	46.051444
3503.612007	376697.959297	46.056449
3503.753335	376692.748178	46.061453
3503.589507	376710.884877	46.066458
3503.547260	376702.497816	46.071463
3503.837374	376706.496525	46.076468
3503.370396	376715.295180	46.081473
3504.033615	376708.424516	46.086477
3503.931954	376714.367437	46.091482
3503.726945	376716.053411	46.096487
3503.669887	376714.968886	46.101492
3503.725840	376723.684873	46.106497
3503.826854	376708.280208	46.111501
3503.642766	376712.328443	46.116506
3503.592417	376708.648363	46.121511
3503.671562	376690.423728	46.126516
3503.393909	376686.118237	46.131521
3503.804019	376679.872613	46.136525
3503.635504	376683.664027	46.141530
3503.881660	376689.297606	46.146535
3504.178766	376697.212390	46.151540
3504.033980	376685.865496	46.156545
3504.001734	376694.493687	46.161549
3503.540796	376697.924347	46.166554
3503.915870	376687.996011	46.171559
3503.778841	376668.050439	46.176564
3503.508154	376665.804180	46.181569
3503.969367	376657.820810	46.186573
3503.467154	376656.297929	46.191578
3503.630400	376666.446833	46.196583
3503.751596	376654.523723	46.201588
3503.762950	376663.323082	46.206593
3503.985912	376658.684087	46.211597
3503.632026	376658.867423	46.216602
3503.897815	376661.877969	46.221607
3504.001426	376665.244822	46.226612
3503.955029	376660.622972	46.231617
3504.207863	376629.016821	46.236621
3504.102697	376627.024193	46.241626
3503.910141	376629.394981	46.246631
3503.842694	376630.804849	46.251636
3503.760149	376631.123346	46.256641
3503.675247	376617.350521	46.261645
3503.774336	376616.215872	46.266650
3503.923893	376616.828349	46.271655
3503.907883	376604.011207	46.276660
3503.376513	376598.728363	46.281665
3503.797297	376592.709966	46.286669
3503.706008	376596.183944	46.291674
3504.021842	376592.751202	46.296679
3503.818915	376594.436852	46.301684
3503.593844	376601.289568	46.306689
3504.129503	376592.785692	46.311693
3504.046743	376595.953087	46.316698
3504.103315	376582.285067	46.321703
3504.054363	376556.933021	46.326708
3503.857241	376569.377313	46.331713
3504.080164	376559.752797	46.336717
3503.917390	376567.460506	46.341722
3504.137153	376560.100321	46.346727
3503.866292	376530.993328	46.351732
3503.438653	376523.710042	46.356737
3504.003012	376523.442985	46.361741
3503.533922	376528.502873	46.366746
3503.620541	376523.554743	46.371751
3503.715967	376528.601701	46.376756
3503.582798	376528.037928	46.381761
3503.479979	376529.427956	46.386765
3503.447415	376529.077207	46.391770
3503.647994	376536.905537	46.396775
3503.838011	376532.983953	46.401780
3503.711346	376533.919896	46.406785
3503.841847	376523.038165	46.411789
3503.803678	376540.010442	46.416794
3503.812330	376527.672668	46.421799
3503.799916	376505.621537	46.426804
3503.735408	376502.579585	46.431809
3503.585985	376498.889711	46.436813
3503.952180	376498.628544	46.441818
3503.650966	376496.590592	46.446823
3503.899009	376501.257317	46.451828
3503.815519	376503.636308	46.456833
3503.884787	376489.025104	46.461837
3504.002335	376499.028657	46.466842
3503.751411	376500.899953	46.471847
3504.082641	376483.601956	46.476852
3503.669450	376471.458031	46.481857
3503.704824	376466.568868	46.486861
3503.614600	376460.860160	46.491866
3503.897799	376453.261000	46.496871
3504.071540	376465.799315	46.501876
3503.808585	376475.176243	46.506881
3503.994993	376473.569932	46.511885
3503.799654	376466.911259	46.516890
3503.938955	376457.834102	46.521895
3504.131404	376438.243314	46.526900
3503.616520	376433.212205	46.531905
3503.750081	376432.199284	46.536909
3503.987802	376448.721005	46.541914
3503.894379	376440.291106	46.546919
3504.102903	376438.604989	46.551924
3503.846923	376429.844675	46.556929
3503.795917	376399.405576	46.561933
3503.859139	376406.568862	46.566938
3503.418120	376403.789913	46.571943
3503.864918	376400.616252	46.576948
3503.626484	376408.793807	46.581953
3503.662108	376397.850732	46.586957
3503.854860	376405.553142	46.591962
3503.736274	376403.079332	46.596967
3503.864195	376404.305707	46.601972
3503.469057	376410.854666	46.606977
3504.028920	376410.461138	46.611981
3503.845248	376427.125791	46.616986
3503.670417	376397.596539	46.621991
3503.895357	376381.129265	46.626996
3503.675394	376379.612627	46.632001
3503.864313	376365.999922	46.637005
3503.952032	376379.569320	46.642010
3503.887555	376370.804157	46.647015
3503.983645	376369.797158	46.652020
3504.029706	376381.516282	46.657025
3504.249582	376350.016868	46.662029
3503.835365	376352.041166	46.667034
3503.613949	376342.003547	46.672039
3503.864186	376325.684871	46.677044
3503.374595	376337.208883	46.682049
3503.313900	376343.526929	46.687053
3503.362892	376352.066042	46.692058
3503.566562	376339.443017	46.697063
3503.778916	376340.783228	46.702068
3503.407760	376341.274533	46.707073
3503.729532	376351.551076	46.712077
3503.680881	376350.973940	46.717082
3503.767376	376347.475686	46.722087
3503.665107	376351.816260	46.727092
3503.839991	376350.008276	46.732097
3503.785095	376365.202720	46.737101
3503.637587	376355.458658	46.742106
3504.049207	376359.539940	46.747111
3503.852197	376338.382738	46.752116
3503.548421	376335.811017	46.757121
3503.728285	376321.411197	46.762125
3503.672949	376331.594740	46.767130
3503.711185	376327.417329	46.772135
3503.861696	376317.753329	46.777140
3504.188082	376334.286517	46.782145
3503.983366	376331.114098	46.787149
3503.899000	376341.760084	46.792154
3503.505523	376318.039410	46.797159
3503.912375	376316.728920	46.802164
3504.059196	376308.871490	46.807169
3504.183079	376296.032136	46.812173
3503.855114	376294.786933	46.817178
3503.660531	376290.137593	46.822183
3503.955228	376299.807953	46.827188
3503.672655	376299.801962	46.832193
3503.759597	376284.272177	46.837197
3503.765944	376288.671897	46.842202
3503.843552	376271.515648	46.847207
3503.832796	376272.814822	46.852212
3503.699047	376271.869591	46.857217
3503.859906	376267.342114	46.862221
3503.753091	376274.786668	46.867226
3503.432853	376267.511793	46.872231
3503.860136	376266.783111	46.877236
3503.923210	376273.539460	46.882241
3504.186693	376259.228146	46.887245
3503.701295	376265.028302	46.892250
3503.655340	376233.876058	46.897255
3503.800962	376229.096621	46.902260
3503.757261	376240.575610	46.907265
3503.609253	376218.342265	46.912269
3503.825586	376229.424039	46.917274
3503.557871	376228.983278	46.922279
3503.881306	376230.433116	46.927284
3503.626006	376237.672220	46.932289
3503.585103	376230.404054	46.937293
3503.526795	376248.244480	46.942298
3503.530920	376241.503365	46.947303
3503.717300	376241.830225	46.952308
3503.483672	376248.404552	46.957313
3503.953254	376244.769421	46.962317
3503.972572	376240.238880	46.967322
3504.076087	376233.660107	46.972327
3503.821666	376210.553301	46.977332
3503.712522	376208.281479	46.982337
3503.926223	376210.104776	46.987341
3503.831264	376217.878141	46.992346
3503.702645	376210.420345	46.997351
3504.473556	376211.316152	47.002356
3504.037032	376202.355401	47.007361
3503.782862	376191.483517	47.012365
3503.762669	376176.174119	47.017370
3503.525827	376176.262644	47.022375
3503.669771	376170.872988	47.027380
3503.990042	376175.223095	47.032385
3504.243834	376176.226086	47.037389
3504.098863	376174.621276	47.042394
3503.847077	376169.599416	47.047399
3503.655897	376145.287057	47.052404
3503.521054	376146.631288	47.057409
3503.760199	376136.393628	47.062413
3503.822135	376144.243952	47.067418
3503.589235	376145.298444	47.072423
3503.627757	376134.380275	47.077428
3503.478813	376146.995137	47.082433
3503.645907	376144.374404	47.087437
3503.528060	376147.089523	47.092442
3503.405710	376150.949998	47.097447
3503.938761	376143.870888	47.102452
3503.641244	376145.062777	47.107457
3503.716248	376144.466091	47.112461
3503.546223	376153.701220	47.117466
3503.582373	376150.160034	47.122471
3503.914712	376146.317661	47.127476
3503.676027	376148.568586	47.132481
3503.862104	376155.661622	47.137485
3503.488866	376162.461526	47.142490
3504.024610	376159.502715	47.147495
3504.283349	376129.039883	47.152500
3503.843764	376132.289158	47.157505
3503.994588	376107.642910	47.162509
3504.095795	376118.437675	47.167514
3503.840549	376124.964567	47.172519
3504.064485	376112.541759	47.177524
3503.775456	376108.441497	47.182529
3503.973267	376088.926001	47.187533
3504.088429	376093.715527	47.192538
3503.720750	376104.075686	47.197543
3504.067201	376099.035557	47.202548
3503.540178	376094.108071	47.207553
3503.913104	376093.108176	47.212557
3503.822572	376076.512592	47.217562
3504.093901	376052.203373	47.222567
3504.332536	376056.617272	47.227572
3503.978096	376060.794248	47.232577
3504.162345	376048.581188	47.237581
3503.763670	376044.091265	47.242586
3503.771963	376017.788676	47.247591
3503.723630	376007.901669	47.252596
3503.787761	376019.363675	47.257601
3503.868158	376013.119197	47.262605
3503.679925	376013.988575	47.267610
3503.812777	376017.834157	47.272615
3503.962432	376012.621634	47.277620
3503.316803	376025.925531	47.282625
3503.565410	376018.382631	47.287629
3503.787945	376009.343088	47.292634
3503.574976	376020.569095	47.297639
3503.897772	376019.831489	47.302644
3504.047729	376014.161058	47.307649
3503.910974	375990.018059	47.312653
3503.832101	375988.555413	47.317658
3503.682314	375981.635091	47.322663
3504.050831	375982.899755	47.327668
3503.630475	375984.136504	47.332673
3503.780845	375982.256069	47.337677
3503.632171	375985.001507	47.342682
3503.578575	375984.348838	47.347687
3503.746290	375980.786840	47.352692
3503.410456	375987.682607	47.357697
3503.583502	375993.073474	47.362701
3503.559500	375992.365254	47.367706
3503.575945	375983.358284	47.372711
3503.980694	375985.863617	47.377716
3503.938300	375977.069441	47.382721
3503.688815	375959.099919	47.387725
3503.867433	375947.218396	47.392730
3503.582231	375959.396996	47.397735
3503.415409	375961.255021	47.402740
3503.472689	375958.499016	47.407745
3503.626120	375960.179232	47.412749
3503.404240	375965.352730	47.417754
3503.345223	375957.146221	47.422759
3503.970946	375957.251011	47.427764
3503.537166	375968.104951	47.432769
3503.742765	375962.018731	47.437773
3504.022648	375973.319460	47.442778
3503.855615	375971.082212	47.447783
3503.972586	375967.451924	47.452788
3503.684192	375963.020869	47.457793
3503.740893	375971.864084	47.462797
3503.749394	375956.600940	47.467802
3503.869663	375949.866853	47.472807
3503.705297	375934.758211	47.477812
3503.516407	375927.793189	47.482817
3503.715887	375935.392879	47.487821
3503.565976	375923.614156	47.492826
3503.981245	375908.286692	47.497831
3503.696662	375910.697506	47.502836
3503.830031	375911.236243	47.507841
3503.822831	375907.778199	47.512845
3504.034359	375911.000873	47.517850
3503.587801	375919.771035	47.522855
3503.820530	375904.116311	47.527860
3503.543103	375898.208185	47.532865
3503.700597	375896.886227	47.537869
3503.650926	375890.916659	47.542874
3503.956790	375898.804780	47.547879
3503.950909	375897.763016	47.552884
3503.869787	375899.709243	47.557889
3504.147738	375879.875737	47.562893
3503.768424	375898.402981	47.567898
3503.561087	375896.680835	47.572903
3504.165783	375889.539481	47.577908
3503.704048	375889.765305	47.582913
3503.520178	375872.039740	47.587917
3504.196787	375864.429152	47.592922
3503.772103	375868.439195	47.597927
3504.072337	375864.042261	47.602932
3503.479333	375874.565282	47.607937
3503.559108	375872.416197	47.612941
3503.704334	375866.975425	47.617946
3503.796611	375884.359781	47.622951
3504.243729	375864.931951	47.627956
3503.804221	375866.171731	47.632961
3503.978706	375851.721721	47.637965
3503.799644	375841.219421	47.642970
3503.682169	375849.047290	47.647975
3504.191101	375852.019460	47.652980
3503.330392	375846.178096	47.657985
3503.891405	375835.838606	47.662989
3503.587558	375846.621165	47.667994
3503.566055	375845.912547	47.672999
3504.075954	375839.218595	47.678004
3503.853161	375837.575200	47.683009
3503.628718	375820.771749	47.688013
3503.898196	375812.513282	47.693018
3504.012706	375808.196576	47.698023
3503.881818	375801.654788	47.703028
3503.601972	375812.026573	47.708033
3504.031585	375808.397722	47.713037
3503.705931	375811.222023	47.718042
3503.317222	375811.817856	47.723047
3503.693491	375811.427908	47.728052
3503.631722	375816.220000	47.733057
3503.665590	375806.676064	47.738061
3503.571363	375814.602012	47.743066
3503.622088	375813.576734	47.748071
3504.022889	375810.079621	47.753076
3503.646704	375794.851791	47.758081
3503.848658	375779.151010	47.763085
3503.719428	375783.343286	47.768090
3503.489097	375786.813877	47.773095
3503.980571	375768.930634	47.778100
3503.788902	375783.205756	47.783105
3503.650349	375783.863791	47.788109
3503.793129	375790.327815	47.793114
3503.986433	375772.593456	47.798119
3503.949478	375777.635997	47.803124
3503.594292	375762.760951	47.808129
3503.575066	375750.401909	47.813133
3503.754196	375748.466042	47.818138
3503.278166	375750.169463	47.823143
3503.470915	375745.891255	47.828148
3503.818748	375750.109867	47.833153
3503.558958	375753.432497	47.838157
3503.706338	375752.926112	47.843162
3503.963459	375757.082753	47.848167
3504.035401	375759.233721	47.853172
3504.001141	375764.606517	47.858177
3504.284983	375757.922850	47.863181
3504.153055	375749.804136	47.868186
3503.517099	375735.838316	47.873191
3504.159513	375725.791172	47.878196
3503.951753	375715.878423	47.883201
3503.754854	375721.048003	47.888205
3503.761077	375720.589368	47.893210
3504.125699	375727.756002	47.898215
3503.865651	375710.652893	47.903220
3503.262440	375693.120723	47.908225
3503.728233	375681.346346	47.913229
3503.979267	375684.003182	47.918234
3503.796970	375689.755505	47.923239
3503.922866	375677.017384	47.928244
3503.811820	375694.026974	47.933249
3503.823117	375697.866365	47.938253
3503.379190	375691.297735	47.943258
3503.364256	375695.141273	47.948263
3503.822506	375680.290228	47.953268
3503.517084	375702.290730	47.958273
3503.813325	375697.004121	47.963277
3504.018954	375691.502902	47.968282
3503.928078	375698.766984	47.973287
3503.949046	375675.336532	47.978292
3503.386662	375674.789725	47.983297
3503.299736	375669.131257	47.988301
3503.893682	375666.290395	47.993306
3503.447746	375664.656830	47.998311
3503.616925	375655.091469	48.003316
3503.449842	375659.238868	48.008321
3503.644414	375659.767934	48.013325
3503.515231	375661.365653	48.018330
3503.152212	375669.715673	48.023335
3503.408472	375672.651489	48.028340
3503.771772	375693.172693	48.033345
3504.020479	375688.631265	48.038349
3503.777029	375666.565325	48.043354
3503.526449	375666.656023	48.048359
3503.730950	375660.340998	48.053364
3503.273400	375666.213148	48.058369
3503.749318	375673.158703	48.063373
3503.526996	375677.111338	48.068378
3503.801953	375671.904400	48.073383
3503.553397	375673.342932	48.078388
3503.653281	375676.049099	48.083393
3503.764077	375674.836264	48.088397
3503.538591	375681.689201	48.093402
3503.545383	375677.847373	48.098407
3503.955275	375677.604731	48.103412
3503.371001	375687.515935	48.108417
3503.624600	375677.453933	48.113421
3503.772931	375686.231852	48.118426
3503.646418	375677.476345	48.123431
3503.877297	375671.564143	48.128436
3503.692692	375691.536039	48.133441
3503.744177	375672.959202	48.138445
3503.781218	375658.607161	48.143450
3503.437647	375642.534701	48.148455
3503.590181	375646.835071	48.153460
3503.724004	375643.532770	48.158465
3503.620292	375650.061220	48.163469
3503.823051	375639.447634	48.168474
3503.535580	375652.542413	48.173479
3504.149891	375640.922604	48.178484
3503.915248	375659.757767	48.183489
3503.529988	375647.558304	48.188493
3503.856447	375643.793123	48.193498
3503.759538	375651.999332	48.198503
3504.071888	375651.950167	48.203508
3503.971991	375645.759571	48.208513
3503.891852	375626.033423	48.213517
3504.069750	375617.763956	48.218522
3503.839692	375620.191605	48.223527
3503.948275	375621.700867	48.228532
3503.756311	375632.007932	48.233537
3503.738045	375623.871224	48.238541
3503.995838	375611.239416	48.243546
3503.779124	375603.541066	48.248551
3503.918693	375581.439968	48.253556
3503.750270	375586.986617	48.258561
3503.661879	375593.639839	48.263565
3503.699006	375587.987185	48.268570
3503.847729	375591.753988	48.273575
3503.766192	375584.237760	48.278580
3503.841935	375579.367546	48.283585
3503.778693	375585.762424	48.288589
3504.185933	375580.076698	48.293594
3503.370981	375560.415804	48.298599
3503.870240	375543.981137	48.303604
3503.528498	375540.906627	48.308609
3503.536931	375538.361811	48.313613
3503.702839	375533.121220	48.318618
3503.472243	375545.825488	48.323623
3503.825321	375534.526751	48.328628
3503.565618	375546.548822	48.333633
3503.572768	375547.209265	48.338637
3503.619729	375549.364194	48.343642
3503.513593	375557.673628	48.348647
3503.759372	375546.213798	48.353652
3503.768099	375560.253824	48.358657
3503.705294	375553.370553	48.363661
3503.484244	375559.179895	48.368666
3503.705197	375550.013316	48.373671
3503.459013	375544.074762	48.378676
3503.274954	375558.806625	48.383681
3503.751551	375544.537680	48.388685
3503.728468	375558.837105	48.393690
3503.405751	375554.691237	48.398695
3503.663388	375558.695195	48.403700
3503.758602	375553.338598	48.408705
3503.490327	375558.163364	48.413709
3503.688227	375553.019467	48.418714
3503.494937	375568.490457	48.423719
3503.554268	375552.532328	48.428724
3503.517590	375574.185173	48.433729
3503.977111	375567.499140	48.438733
3504.058334	375559.372129	48.443738
3503.905769	375557.921116	48.448743
3503.818405	375528.326528	48.453748
3503.675282	375530.231700	48.458753
3503.845367	375531.909301	48.463757
3504.181264	375535.290403	48.468762
3503.872154	375527.555771	48.473767
3504.033297	375535.212471	48.478772
3503.570988	375512.341624	48.483777
3503.493791	375490.681735	48.488781
3503.555380	375500.948751	48.493786
3503.395550	375500.414616	48.498791
3503.835115	375503.779333	48.503796
3503.469985	375495.773743	48.508801
3503.566709	375503.898498	48.513805
3503.532665	375496.959797	48.518810
3503.234159	375502.806828	48.523815
3503.837871	375498.412755	48.528820
3503.675662	375512.835937	48.533825
3503.772317	375505.927450	48.538829
3503.824526	375504.545813	48.543834
3503.419302	375501.150654	48.548839
3503.782667	375506.435190	48.553844
3503.776440	375510.964168	48.558849
3503.718902	375509.345509	48.563853
3503.814324	375502.411780	48.568858
3503.731231	375514.914681	48.573863
3503.670045	375507.471533	48.578868
3503.569684	375510.183929	48.583873
3503.752307	375499.802423	48.588877
3503.659709	375505.260786	48.593882
3503.707727	375508.967205	48.598887
3503.867357	375494.315921	48.603892
3503.630760	375480.159697	48.608897
3503.533956	375468.652253	48.613901
3503.824934	375478.908450	48.618906
3503.813722	375468.913695	48.623911
3504.031962	375465.750657	48.628916
3503.567102	375480.806745	48.633921
3503.860213	375475.215357	48.638925
3503.866496	375485.389372	48.643930
3503.327850	375493.029519	48.648935
3503.664912	375483.920881	48.653940
3503.603294	375494.792426	48.658945
3503.950708	375490.184498	48.663949
3503.699105	375479.210268	48.668954
3503.634117	375475.634138	48.673959
3504.025794	375468.297452	48.678964
3503.744837	375446.924121	48.683969
3503.678692	375432.486564	48.688973
3504.007081	375432.104183	48.693978
3503.587963	375426.421882	48.698983
3503.771582	375422.730136	48.703988
3503.909413	375429.754615	48.708993
3503.598307	375425.047284	48.713997
3503.514484	375449.378536	48.719002
3503.764587	375442.089662	48.724007
3504.080563	375442.853909	48.729012
3503.844915	375437.982029	48.734017
3503.242990	375435.533692	48.739021
3503.950701	375419.269518	48.744026
3503.571419	375416.938607	48.749031
3503.697277	375408.041399	48.754036
3503.576424	375424.772845	48.759041
3503.489063	375410.313197	48.764045
3503.884409	375408.139638	48.769050
3503.434239	375416.706983	48.774055
3504.009167	375410.511421	48.779060
3503.526325	375412.444865	48.784065
3503.804444	375413.800149	48.789069
3503.738324	375416.354516	48.794074
3503.793773	375416.371400	48.799079
3503.775469	375415.229839	48.804084
3503.843785	375416.567414	48.809089
3503.755337	375418.260452	48.814093
3503.901398	375421.646137	48.819098
3503.486062	375406.449787	48.824103
3503.793833	375390.630380	48.829108
3503.471784	375389.257027	48.834113
3503.421055	375397.506861	48.839117
3503.701233	375378.079751	48.844122
3503.536705	375384.032806	48.849127
3503.651417	375379.410777	48.854132
3503.773849	375385.165846	48.859137
3503.554235	375371.770010	48.864141
3503.730131	375376.626331	48.869146
3503.516276	375385.410696	48.874151
3503.837634	375382.434846	48.879156
3503.568328	375396.391696	48.884161
3503.517217	375401.436522	48.889165
3503.687037	375390.268463	48.894170
3503.292651	375403.253038	48.899175
3503.738042	375391.481803	48.904180
3503.515642	375403.752389	48.909185
3503.729508	375390.186287	48.914189
3504.029055	375386.196403	48.919194
3503.763382	375399.694810	48.924199
3503.833968	375384.345325	48.929204
3503.823094	375388.976799	48.934209
3503.912446	375383.671980	48.939213
3504.001964	375356.669321	48.944218
3503.967282	375350.697304	48.949223
3503.997737	375353.261846	48.954228
3503.792615	375360.798419	48.959233
3503.591910	375358.490149	48.964237
3504.210823	375348.726436	48.969242
3503.464959	375358.739575	48.974247
3503.524704	375343.417226	48.979252
3503.765309	375337.274504	48.984257
3503.547056	375336.953099	48.989261
3503.421485	375326.772891	48.994266
3503.417901	375329.190193	48.999271
3503.739653	375342.646631	49.004276
3503.910721	375340.940954	49.009281
3504.066145	375325.094731	49.014285
3503.925894	375310.032918	49.019290
3503.558418	375326.396397	49.024295
3504.123592	375319.210318	49.029300
3503.855761	375325.256022	49.034305
3503.675020	375323.605958	49.039309
3503.988424	375319.435818	49.044314
3503.677055	375317.017854	49.049319
3503.858440	375288.957707	49.054324
3503.759557	375289.431419	49.059329
3503.764208	375299.554864	49.064333
3503.567818	375293.862773	49.069338
3503.588674	375294.571927	49.074343
3503.601069	375289.177513	49.079348
3503.420683	375298.974090	49.084353
3503.533045	375285.296812	49.089357
3503.719210	375300.453548	49.094362
3503.568778	375298.925877	49.099367
3503.873855	375294.757051	49.104372
3503.368418	375299.390406	49.109377
3503.725050	375295.951106	49.114381
3503.921727	375288.874148	49.119386
3503.680790	375295.169976	49.124391
3503.933380	375302.405270	49.129396
3504.078418	375285.263381	49.134401
3503.823152	375283.625097	49.139405
3503.674528	375268.004976	49.144410
3503.513871	375275.661721	49.149415
3503.712936	375264.336382	49.154420
3503.608791	375264.581992	49.159425
3503.753871	375270.715053	49.164429
3503.951881	375260.356491	49.169434
3503.554406	375271.713620	49.174439
3503.836147	375277.672454	49.179444
3504.108074	375284.624886	49.184449
3503.802967	375282.180493	49.189453
3503.834533	375248.369776	49.194458
3503.572395	375236.328786	49.199463
3503.776863	375207.985125	49.204468
3503.508872	375209.859177	49.209473
3503.597245	375219.282604	49.214477
3504.057595	375200.615480	49.219482
3503.571848	375222.721059	49.224487
3503.645955	375218.436114	49.229492
3503.448326	375210.836421	49.234497
3503.518820	375215.811172	49.239501
3503.578232	375209.824260	49.244506
3503.465267	375215.235007	49.249511
3503.858886	375218.200017	49.254516
3503.836482	375223.901693	49.259521
3503.259979	375216.997822	49.264525
3503.455913	375221.138754	49.269530
3503.384946	375214.638273	49.274535
3503.516723	375210.649457	49.279540
3503.600435	375225.873291	49.284545
3503.705738	375220.998361	49.289549
3503.821161	375217.190191	49.294554
3503.315108	375234.109794	49.299559
3503.622942	375218.824490	49.304564
3503.599479	375235.591493	49.309569
3503.690415	375229.777660	49.314573
3503.758616	375233.811597	49.319578
3503.714244	375230.537432	49.324583
3503.539637	375234.101009	49.329588
3503.619486	375230.578272	49.334593
3503.500106	375221.109300	49.339597
3503.730773	375235.699407	49.344602
3503.909077	375235.645996	49.349607
3503.859693	375219.781234	49.354612
3503.755671	375203.441797	49.359617
3503.573389	375209.804678	49.364621
3503.387559	375194.419345	49.369626
3503.583059	375204.894201	49.374631
3503.839148	375202.411963	49.379636
3503.538400	375207.241904	49.384641
3503.563711	375203.091857	49.389645
3503.413011	375205.125428	49.394650
3503.412485	375208.585177	49.399655
3503.587271	375199.985435	49.404660
3503.848093	375202.946001	49.409665
3503.590513	375213.645102	49.414669
3503.767696	375195.734979	49.419674
3503.647513	375202.622225	49.424679
3503.572822	375197.979243	49.429684
3503.728021	375208.333284	49.434689
3503.382197	375205.768137	49.439693
3503.561343	375206.961013	49.444698
3503.680026	375200.735796	49.449703
3503.605935	375211.583951	49.454708
3503.694921	375193.586021	49.459713
3503.593593	375212.273130	49.464717
3504.071458	375206.805122	49.469722
3503.787038	375203.925022	49.474727
3503.647655	375213.409892	49.479732
3503.430151	375191.772023	49.484737
3503.619966	375206.444911	49.489741
3503.880105	375197.195746	49.494746
3503.452035	375187.419444	49.499751
3503.701869	375177.383351	49.504756
3503.640747	375164.165890	49.509761
3503.744312	375178.954171	49.514765
3503.913870	375173.229650	49.519770
3503.766906	375170.861999	49.524775
3504.024539	375175.501926	49.529780
3503.861828	375178.071578	49.534785
3503.776219	375172.311083	49.539789
3503.857972	375167.795990	49.544794
3503.527313	375185.145756	49.549799
3503.865603	375173.544011	49.554804
3503.564649	375151.563193	49.559809
3503.182850	375143.585605	49.564813
3503.296928	375160.737891	49.569818
3503.437931	375166.108497	49.574823
3503.928799	375170.584368	49.579828
3503.815555	375178.309948	49.584833
3503.633274	375168.901781	49.589837
3503.912797	375150.466716	49.594842
3503.801306	375151.120483	49.599847
3503.652543	375145.802400	49.604852
3503.459705	375151.759963	49.609857
3503.573153	375149.681828	49.614861
3503.657062	375137.484357	49.619866
3503.506585	375153.686415	49.624871
3503.733634	375150.420211	49.629876
3503.710955	375157.800795	49.634881
3503.551206	375157.775386	49.639885
3503.960372	375143.491523	49.644890
3503.607789	375153.060985	49.649895
3503.719185	375151.568230	49.654900
3504.129082	375156.362148	49.659905
3504.123970	375157.940275	49.664909
3503.965304	375129.781150	49.669914
3503.598432	375123.785302	49.674919
3504.052073	375107.713791	49.679924
3503.730222	375112.979513	49.684929
3503.967954	375120.649620	49.689933
3504.125734	375115.740945	49.694938
3503.949122	375117.295309	49.699943
3503.945013	375093.385179	49.704948
3503.875829	375089.860553	49.709953
3503.685217	375087.398048	49.714957
3503.709414	375083.044668	49.719962
3503.701935	375081.901386	49.724967
3503.697847	375078.773464	49.729972
3503.570541	375093.928956	49.734977
3503.569993	375089.223367	49.739981
3503.998222	375088.316455	49.744986
3503.557747	375099.858490	49.749991
3503.853741	375090.527321	49.754996
3504.138605	375085.445929	49.760001
3503.978358	375063.468257	49.765005
3504.033396	375043.923955	49.770010
3503.719829	375041.684383	49.775015
3503.850716	375045.352307	49.780020
3503.692354	375041.333028	49.785025
3503.644666	375053.805037	49.790029
3503.873462	375047.893074	49.795034
3503.760040	375048.318212	49.800039
3503.759754	375041.323222	49.805044
3503.606575	375021.252205	49.810049
3503.470057	375018.196087	49.815053
3503.890091	375008.260234	49.820058
3503.717008	375013.298952	49.825063
3503.741467	375012.964613	49.830068
3503.756111	375007.315433	49.835073
3503.757314	375017.617554	49.840077
3504.131138	375010.207297	49.845082
3503.518325	375013.534919	49.850087
3503.823263	375016.513962	49.855092
3504.057719	375014.009695	49.860097
3504.020241	375004.705785	49.865101
3503.946894	374982.256461	49.870106
3503.878103	374980.029065	49.875111
3503.911711	374978.446852	49.880116
3504.030625	374981.964051	49.885121
3504.072452	374984.959252	49.890125
3503.780029	374962.035803	49.895130
3503.786331	374956.413372	49.900135
3503.715073	374929.537595	49.905140
3503.774974	374941.102323	49.910145
3503.958001	374938.936866	49.915149
3503.779080	374942.730087	49.920154
3503.989435	374943.943475	49.925159
3503.867036	374935.263470	49.930164
3503.704477	374934.449948	49.935169
3503.712110	374935.008574	49.940173
3503.823087	374934.151811	49.945178
3503.777599	374918.693313	49.950183
3503.558942	374907.001475	49.955188
3503.582108	374905.471784	49.960193
3503.372435	374914.230152	49.965197
3503.353165	374903.829535	49.970202
3503.353675	374918.964887	49.975207
3503.437940	374942.811997	49.980212
3503.423780	374942.331139	49.985217
3503.276644	374959.779175	49.990221
3503.974198	374958.270064	49.995226
3503.694891	374961.519531	50.000231
3503.969105	374945.450884	50.005236
3503.739023	374930.886441	50.010241
3503.792516	374919.991016	50.015245
3503.837452	374917.643889	50.020250
3503.563017	374925.496748	50.025255
3503.698196	374920.769683	50.030260
3503.556790	374919.444070	50.035265
3503.437473	374926.280351	50.040269
3503.802982	374913.173426	50.045274
3503.797638	374923.934479	50.050279
3503.840631	374917.593997	50.055284
3503.849252	374910.979136	50.060289
3503.945058	374919.231340	50.065293
3504.040604	374917.156023	50.070298
3503.443261	374911.552699	50.075303
3503.977228	374903.710110	50.080308
3504.190592	374896.579572	50.085313
3504.033622	374899.911454	50.090317
3504.040454	374894.746803	50.095322
3504.096190	374906.312199	50.100327
3503.910471	374867.422608	50.105332
3503.917037	374865.183293	50.110337
3504.022968	374858.095169	50.115341
3503.970719	374854.771344	50.120346
3503.460905	374859.100191	50.125351
3503.615946	374861.492444	50.130356
3504.053294	374855.598360	50.135361
3503.807637	374866.524603	50.140365
3503.859059	374841.104742	50.145370
3503.717482	374834.360989	50.150375
3503.928489	374825.755442	50.155380
3503.845321	374818.188456	50.160385
3503.830489	374818.725198	50.165389
3504.084419	374811.944356	50.170394
3503.846887	374823.174576	50.175399
3504.045460	374816.377048	50.180404
3503.998353	374801.478385	50.185409
3503.822754	374791.407701	50.190413
3503.613563	374781.774762	50.195418
3503.617361	374789.405601	50.200423
3503.835358	374784.716303	50.205428
3503.951747	374780.704440	50.210433
3503.894805	374780.077718	50.215437
3503.604036	374777.987151	50.220442
3503.449115	374784.523835	50.225447
3503.857849	374785.400618	50.230452
3503.854560	374785.477662	50.235457
3503.225305	374777.768058	50.240461
3503.679165	374773.346723	50.245466
3503.609738	374780.912827	50.250471
3503.670575	374785.380408	50.255476
3503.939081	374768.498596	50.260481
3503.659891	374756.434723	50.265485
3504.001366	374750.097905	50.270490
3503.686894	374746.077838	50.275495
3503.468175	374755.295543	50.280500
3503.361218	374755.388976	50.285505
3503.253032	374754.821229	50.290509
3503.531115	374756.227415	50.295514
3503.524770	374764.088799	50.300519
3503.793534	374751.861990	50.305524
3503.779800	374749.473253	50.310529
3503.440598	374760.846749	50.315533
3503.738932	374749.861700	50.320538
3503.316390	374768.294540	50.325543
3503.618791	374744.208565	50.330548
3503.514462	374754.196749	50.335553
3503.412833	374754.416526	50.340557
3503.713147	374756.200760	50.345562
3503.509196	374756.920024	50.350567
3503.446055	374760.008148	50.355572
3503.603869	374763.875340	50.360577
3503.392437	374768.360527	50.365581
3503.619647	374759.803280	50.370586
3503.539379	374754.779567	50.375591
3503.647347	374755.958271	50.380596
3503.788730	374752.552953	50.385601
3503.711470	374758.110741	50.390605
3503.790794	374762.321029	50.395610
3503.681111	374761.499144	50.400615
3503.753072	374766.143032	50.405620
3503.931580	374765.148402	50.410625
3503.944820	374772.981251	50.415629
3504.055944	374738.470724	50.420634
3503.538915	374737.331672	50.425639
3503.509744	374728.687760	50.430644
3503.810736	374728.182516	50.435649
3503.602326	374724.934242	50.440653
3503.833759	374723.854932	50.445658
3503.560400	374730.079661	50.450663
3503.732515	374728.679042	50.455668
3503.844380	374735.936682	50.460673
3503.475132	374738.589886	50.465677
3503.426027	374729.872814	50.470682
3503.616252	374730.046454	50.475687
3503.506289	374737.847911	50.480692
3503.677682	374731.232728	50.485697
3503.657525	374731.007189	50.490701
3503.891775	374732.598368	50.495706
3503.840540	374732.784741	50.500711
3504.079904	374731.042805	50.505716
3503.894758	374706.423381	50.510721
3503.637476	374695.856837	50.515725
3503.963247	374698.807173	50.520730
3503.679174	374693.510421	50.525735
3503.308438	374666.249376	50.530740
3503.782766	374627.662216	50.535745
3503.252656	374597.144878	50.540749
3503.581374	374541.384873	50.545754
3503.034134	374491.410415	50.550759
3503.032522	374415.148867	50.555764
3502.802611	374338.516264	50.560769
3502.630676	374269.912681	50.565773
3502.254171	374170.663341	50.570778
3501.769493	374079.520102	50.575783
3501.655022	373981.882344	50.580788
3501.031177	373875.167205	50.585793
3500.790114	373767.500946	50.590797
3501.016366	373655.054479	50.595802
3500.197064	373533.538927	50.600807
3500.163639	373412.763685	50.605812
3499.654414	373262.325871	50.610817
3498.787159	373135.271169	50.615821
3498.567317	372994.198860	50.620826
3498.211140	372855.971311	50.625831
3497.793467	372711.266158	50.630836
3497.329736	372548.048343	50.635841
3496.767783	372392.375331	50.640845
3496.569636	372231.683626	50.645850
3495.704210	372082.340869	50.650855
3495.342676	371911.879722	50.655860
3495.397735	371739.037052	50.660865
3494.739243	371568.188992	50.665869
3494.237027	371390.141598	50.670874
3493.515835	371203.300529	50.675879
3493.203545	371013.112270	50.680884
3492.262080	370842.789375	50.685889
3491.962783	370652.470250	50.690893
3491.767968	370455.214065	50.695898
3490.522634	370270.410647	50.700903
3490.196202	370068.238093	50.705908
3489.706546	369873.086502	50.710913
3488.828697	369695.345825	50.715917
3488.489289	369486.354531	50.720922
3487.984793	369284.689821	50.725927
3487.390384	369088.711699	50.730932
3486.654479	368880.085451	50.735937
3485.915833	368677.513619	50.740941
3485.818326	368463.390935	50.745946
3484.661646	368266.709324	50.750951
3484.207359	368070.984328	50.755956
3483.644019	367858.865881	50.760961
3482.796523	367652.235859	50.765965
3482.277158	367453.592606	50.770970
3481.637471	367247.436671	50.775975
3480.951868	367023.197731	50.780980
3480.376705	366806.318432	50.785985
3479.874708	366616.064601	50.790989
3479.345248	366386.073246	50.795994
3478.220973	366189.580809	50.800999
3477.843634	365969.384080	50.806004
3477.333612	365752.209497	50.811009
3476.766966	365526.239571	50.816013
3476.173288	365320.423669	50.821018
3475.486166	365107.370307	50.826023
3474.451073	364884.906058	50.831028
3474.018954	364665.754808	50.836033
3472.984620	364452.880485	50.841037
3472.745313	364236.088378	50.846042
3471.873472	364023.593464	50.851047
3471.323729	363800.436547	50.856052
3470.957251	363582.745478	50.861057
3469.913291	363358.646794	50.866061
3469.168022	363143.583395	50.871066
3468.430156	362921.724183	50.876071
3467.860344	362712.610472	50.881076
3467.136075	362493.495070	50.886081
3466.317609	362289.736693	50.891085
3465.974884	362068.243509	50.896090
3465.082752	361851.263559	50.901095
3464.287350	361637.804179	50.906100
3464.144003	361409.965997	50.911105
3463.139432	361198.166190	50.916109
3462.407940	360973.650445	50.921114
3461.569947	360773.679969	50.926119
3461.055549	360553.173755	50.931124
3460.398232	360338.617980	50.936129
3459.729697	360127.192858	50.941133
3459.268494	359916.268391	50.946138
3458.260708	359707.515994	50.951143
3457.789897	359478.371725	50.956148
3457.076755	359263.311055	50.961153
3456.203549	359051.811792	50.966157
3455.553869	358835.186960	50.971162
3454.819568	358614.375843	50.976167
3454.299623	358418.722142	50.981172
3453.650127	358198.684591	50.986177
3452.846251	357987.475120	50.991181
3452.458469	357773.170752	50.996186
3451.687369	357552.666045	51.001191
3450.649421	357339.276900	51.006196
3450.530050	357129.380588	51.011201
3449.508868	356931.586313	51.016205
3448.976247	356700.326706	51.021210
3448.164217	356489.544756	51.026215
3447.407548	356286.311182	51.031220
3446.973044	356062.133070	51.036225
3446.219146	355847.776522	51.041229
3445.595350	355640.574883	51.046234
3444.839214	355423.952005	51.051239
3444.269938	355217.376225	51.056244
3443.828586	354997.291676	51.061249
3442.904624	354786.571226	51.066253
3442.258497	354565.321109	51.071258
3441.270462	354357.764669	51.076263
3441.027856	354142.963833	51.081268
3440.579024	353924.148313	51.086273
3439.493067	353719.353284	51.091277
3438.929308	353508.876049	51.096282
3438.037798	353290.026051	51.101287
3437.325196	353081.911966	51.106292
3436.651036	352870.406184	51.111297
3436.132987	352656.889795	51.116301
3435.455077	352442.252576	51.121306
3434.680583	352235.900958	51.126311
3433.979417	352026.253898	51.131316
3433.706461	351806.409180	51.136321
3432.463369	351607.178875	51.141325
3431.841825	351387.234842	51.146330
3431.445402	351188.047256	51.151335
3430.567144	350968.752904	51.156340
3430.563815	350762.757216	51.161345
3429.429460	350550.118796	51.166349
3428.951452	350339.030062	51.171354
3428.007291	350133.257088	51.176359
3427.364050	349909.034715	51.181364
3426.936404	349697.299254	51.186369
3426.142241	349498.779172	51.191373
3425.476132	349271.401859	51.196378
3424.901003	349062.512357	51.201383
3424.046381	348852.240976	51.206388
3423.534100	348641.431087	51.211393
3422.753888	348433.157022	51.216397
3422.387906	348216.901191	51.221402
3421.401989	348010.185176	51.226407
3420.663809	347792.459444	51.231412
3420.162058	347569.503270	51.236417
3419.044691	347372.884696	51.241421
3418.734767	347155.546925	51.246426
3417.910749	346948.775962	51.251431
3417.164558	346736.290601	51.256436
3416.801759	346534.153898	51.261441
3415.800818	346330.106629	51.266445
3415.205153	346109.552119	51.271450
3414.317862	345915.488310	51.276455
3413.872320	345696.919250	51.281460
3413.267962	345481.988797	51.286465
3412.052528	345283.418672	51.291469
3411.832496	345082.450599	51.296474
3411.135767	344882.066274	51.301479
3410.363366	344675.329900	51.306484
3409.419863	344468.798026	51.311489
3408.957479	344262.545701	51.316493
3408.661122	344056.851835	51.321498
3407.742834	343865.713279	51.326503
3406.757694	343658.014287	51.331508
3406.660116	343439.814512	51.336513
3405.616514	343245.079333	51.341517
3405.056443	343045.685340	51.346522
3403.952506	342842.176758	51.351527
3403.474821	342633.935801	51.356532
3403.070059	342430.544362	51.361537
3402.250542	342234.777767	51.366541
3401.924010	342021.267208	51.371546
3400.663599	341824.219926	51.376551
3400.480697	341638.888926	51.381556
3400.048579	341419.614769	51.386561
3399.119631	341213.222147	51.391565
3398.299524	340995.076933	51.396570
3397.565938	340802.143126	51.401575
3397.354750	340597.289527	51.406580
3396.455966	340387.452960	51.411585
3395.838788	340186.429568	51.416589
3394.991740	339985.823711	51.421594
3394.396790	339781.384501	51.426599
3393.607372	339573.513440	51.431604
3393.022313	339364.183871	51.436609
3392.224886	339171.611530	51.441613
3391.723836	338958.525369	51.446618
3391.127656	338757.239564	51.451623
3390.321849	338555.960820	51.456628
3389.699239	338346.837506	51.461633
3388.766915	338149.472257	51.466637
3388.581893	337932.107025	51.471642
3387.903606	337743.711828	51.476647
3387.318277	337532.950800	51.481652
3386.595636	337327.327530	51.486657
3385.704276	337131.581926	51.491661
3385.037165	336918.718977	51.496666
3384.544695	336717.894138	51.501671
3383.921091	336511.590793	51.506676
3383.412057	336310.665516	51.511681
3382.366796	336104.274847	51.516685
3381.879520	335892.449360	51.521690
3381.130430	335687.257960	51.526695
3380.525792	335481.864893	51.531700
3380.163623	335280.251427	51.536705
3379.097278	335069.304099	51.541709
3378.561601	334860.894299	51.546714
3377.790462	334665.198857	51.551719
3376.855022	334464.513726	51.556724
3376.279761	334248.674759	51.561729
3375.511278	334051.500616	51.566733
3375.153362	333839.062773	51.571738
3374.404700	333642.113451	51.576743
3373.617721	333443.998575	51.581748
3373.014052	333250.436564	51.586753
3372.162950	333049.937676	51.591757
3371.591919	332845.371561	51.596762
3370.730918	332644.134804	51.601767
3370.315129	332449.471647	51.606772
3369.977514	332244.739599	51.611777
3368.530943	332046.114117	51.616781
3368.544394	331837.481185	51.621786
3367.853721	331640.949923	51.626791
3366.861225	331437.999396	51.631796
3366.621183	331234.776557	51.636801
3365.564467	331039.676315	51.641805
3365.118255	330830.654922	51.646810
3364.648509	330628.943328	51.651815
3363.839812	330431.078153	51.656820
3363.225850	330223.583636	51.661825
3362.115343	330024.975876	51.666829
3361.545445	329811.846802	51.671834
3360.999217	329622.084865	51.676839
3359.826108	329427.635255	51.681844
3359.279092	329220.178280	51.686849
3358.919978	329026.031714	51.691853
3358.282624	328818.740680	51.696858
3357.508114	328637.821324	51.701863
3357.050238	328455.349353	51.706868
3356.637071	328231.599874	51.711873
3355.632953	328026.248705	51.716877
3355.004439	327818.826269	51.721882
3354.448419	327621.270218	51.726887
3353.411750	327426.208365	51.731892
3352.830495	327222.799525	51.736897
3352.137137	327033.640024	51.741901
3351.489587	326835.561804	51.746906
3350.623278	326649.534860	51.751911
3350.263560	326446.903706	51.756916
3349.427025	326254.837064	51.761921
3348.616482	326057.419186	51.766925
3348.184640	325856.351019	51.771930
3347.644658	325671.721430	51.776935
3346.927051	325472.734334	51.781940
3346.193700	325268.631669	51.786945
3345.491058	325059.584275	51.791949
3344.898820	324869.105184	51.796954
3344.057243	324674.031230	51.801959
3343.545318	324473.379686	51.806964
3343.269797	324277.400527	51.811969
3342.171538	324085.726614	51.816973
3341.609090	323878.487245	51.821978
3341.026567	323684.031983	51.826983
3340.213936	323480.421204	51.831988
3339.488580	323293.880572	51.836993
3338.743971	323094.942962	51.841997
3338.114556	322891.556406	51.847002
3337.756758	322705.618349	51.852007
3336.833586	322501.971790	51.857012
3336.323331	322298.845059	51.862017
3335.212934	322102.356376	51.867021
3334.767228	321914.826444	51.872026
3333.979991	321716.274317	51.877031
3333.701232	321522.097117	51.882036
3333.001468	321325.821825	51.887041
3332.341249	321130.736547	51.892045
3331.749745	320932.329932	51.897050
3331.181662	320731.194747	51.902055
3330.096941	320530.522749	51.907060
3329.513198	320334.863475	51.912065
3328.812649	320148.006667	51.917069
3328.205430	319947.614323	51.922074
3327.639144	319749.455737	51.927079
3326.890477	319560.568360	51.932084
3326.220778	319366.677496	51.937089
3325.380414	319157.383035	51.942093
3324.711612	318960.257459	51.947098
3324.108667	318775.470341	51.952103
3323.496438	318587.119576	51.957108
3322.870361	318379.444543	51.962113
3321.811592	318198.776931	51.967117
3321.471536	318003.685289	51.972122
3320.893766	317805.346154	51.977127
3320.405366	317621.506250	51.982132
3319.722207	317420.356620	51.987137
3318.656780	317225.887377	51.992141
3318.293644	317022.954832	51.997146
3317.763612	316839.858452	52.002151
3316.963478	316642.137752	52.007156
3316.354034	316435.143399	52.012161
3315.333416	316241.479932	52.017165
3314.704073	316056.462608	52.022170
3313.963282	315862.703221	52.027175
3313.126452	315663.942385	52.032180
3312.689096	315465.168901	52.037185
3312.010654	315293.475254	52.042189
3311.548356	315088.415526	52.047194
3311.037206	314897.546264	52.052199
3310.223525	314704.050827	52.057204
3309.644657	314508.098850	52.062209
3308.567528	314315.128162	52.067213
3308.352165	314127.673746	52.072218
3307.380550	313930.407765	52.077223
3306.558876	313747.173686	52.082228
3306.263770	313548.297630	52.087233
3305.233769	313363.949969	52.092237
3304.854979	313174.737244	52.097242
3304.119096	312971.753754	52.102247
3303.372027	312790.135925	52.107252
3303.177870	312587.575311	52.112257
3302.142646	312393.550491	52.117261
3301.670987	312207.151815	52.122266
3300.840063	312012.177300	52.127271
3300.263215	311818.282680	52.132276
3299.923896	311615.896024	52.137281
3298.917632	311429.045850	52.142285
3298.224837	311226.332437	52.147290
3297.442811	311042.323624	52.152295
3296.731938	310839.306807	52.157300
3296.215545	310650.824539	52.162305
3295.494171	310464.360615	52.167309
3294.840839	310256.673664	52.172314
3294.223241	310069.785258	52.177319
3293.180150	309880.875755	52.182324
3292.663652	309681.875042	52.187329
3291.662515	309505.614242	52.192333
3291.255469	309309.549498	52.197338
3290.959566	309118.254232	52.202343
3289.843560	308942.265418	52.207348
3289.200598	308751.661087	52.212353
3288.719141	308558.789999	52.217357
3288.302259	308375.126703	52.222362
3287.562920	308190.775653	52.227367
3286.681570	307997.432171	52.232372
3286.006259	307795.423142	52.237377
3285.223601	307623.836100	52.242381
3284.668222	307427.766341	52.247386
3283.825524	307240.119770	52.252391
3283.448979	307056.448156	52.257396
3282.931626	306865.744677	52.262401
3282.156414	306679.130683	52.267405
3281.540342	306478.077873	52.272410
3280.814254	306297.643636	52.277415
3280.279860	306104.446129	52.282420
3279.500640	305913.859074	52.287425
3279.063418	305723.294045	52.292429
3278.212757	305525.740194	52.297434
3277.763794	305339.123631	52.302439
3276.740398	305151.451721	52.307444
3275.784940	304974.820883	52.312449
3275.422551	304789.896068	52.317453
3274.869995	304604.109786	52.322458
3274.044722	304419.767007	52.327463
3273.329298	304231.433952	52.332468
3273.257486	304034.391402	52.337473
3271.924873	303855.679676	52.342477
3271.269312	303666.699753	52.347482
3270.669882	303474.527467	52.352487
3270.125088	303271.981652	52.357492
3269.301479	303076.355466	52.362497
3268.739916	302901.747940	52.367501
3268.064962	302705.664823	52.372506
3267.562276	302520.555532	52.377511
3266.424610	302333.025312	52.382516
3266.189289	302145.759580	52.387521
3265.345919	301967.528417	52.392525
3264.613024	301769.237688	52.397530
3264.133683	301599.148621	52.402535
3263.247864	301402.154920	52.407540
3262.724353	301217.785860	52.412545
3262.202261	301033.161696	52.417549
3261.389131	300831.189850	52.422554
3260.699670	300654.639080	52.427559
3259.853781	300476.508478	52.432564
3259.474203	300273.652422	52.437569
3258.547213	300090.619205	52.442573
3258.033817	299901.663069	52.447578
3257.477859	299716.762623	52.452583
3256.128802	299543.090839	52.457588
3255.921971	299348.584808	52.462593
3255.219508	299168.494646	52.467597
3254.646004	298989.428024	52.472602
3253.930669	298806.818322	52.477607
3253.136688	298624.399133	52.482612
3252.981656	298438.924542	52.487617
3251.831906	298255.440712	52.492621
3251.178587	298081.504593	52.497626
3250.507293	297891.374279	52.502631
3249.525536	297720.927780	52.507636
3248.845836	297531.587886	52.512641
3248.105524	297360.440717	52.517645
3248.155666	297181.375482	52.522650
3247.353743	296990.908357	52.527655
3246.607877	296803.641003	52.532660
3246.093776	296628.433602	52.537665
3245.331573	296444.530114	52.542669
3244.479930	296262.703426	52.547674
3244.247975	296083.019635	52.552679
3243.334192	295897.789854	52.557684
3242.847687	295710.378539	52.562689
3242.208136	295525.105028	52.567693
3241.747798	295344.005069	52.572698
3240.812315	295156.435057	52.577703
3239.828584	294974.628085	52.582708
3239.185447	294784.744908	52.587713
3238.758246	294605.701897	52.592717
3237.843225	294423.043155	52.597722
3237.659650	294236.804999	52.602727
3236.810660	294054.823111	52.607732
3236.250094	293868.262263	52.612737
3235.434259	293696.487216	52.617741
3235.039598	293504.042330	52.622746
3234.088389	293315.836501	52.627751
3232.763882	293137.469043	52.632756
3232.926951	292941.522815	52.637761
3232.037189	292774.164618	52.642765
3231.269872	292574.239540	52.647770
3230.439412	292409.571248	52.652775
3229.439462	292232.959940	52.657780
3229.229995	292047.589966	52.662785
3227.972888	291876.698330	52.667789
3227.523811	291691.849873	52.672794
3227.156513	291522.192471	52.677799
3226.261653	291349.409499	52.682804
3225.926315	291157.768279	52.687809
3225.195104	290983.762192	52.692813
3224.669660	290810.793075	52.697818
3224.006497	290626.843609	52.702823
3223.201896	290451.397121	52.707828
3222.716781	290268.947299	52.712833
3221.715656	290103.031118	52.717837
3221.364388	289917.300020	52.722842
3220.667536	289739.110981	52.727847
3219.722397	289559.509447	52.732852
3219.364805	289373.931795	52.737857
3218.384544	289210.431220	52.742861
3218.060280	289034.780510	52.747866
3217.336258	288848.700201	52.752871
3216.749767	288674.516958	52.757876
3216.502038	288484.235286	52.762881
3215.610910	288305.923301	52.767885
3214.442989	288114.029696	52.772890
3213.999174	287940.180016	52.777895
3213.069243	287760.906083	52.782900
3212.903042	287579.270048	52.787905
3211.697403	287406.177303	52.792909
3211.252041	287223.362777	52.797914
3210.817181	287038.483587	52.802919
3209.650074	286863.678116	52.807924
3209.719844	286685.111360	52.812929
3208.659765	286514.923955	52.817933
3208.084090	286327.570805	52.822938
3207.671788	286149.436601	52.827943
3206.559918	285973.424962	52.832948
3206.270130	285781.467531	52.837953
3205.433521	285608.773956	52.842957
3204.634671	285426.702084	52.847962
3203.878302	285245.718536	52.852967
3203.412161	285077.448500	52.857972
3202.673259	284888.261306	52.862977
3201.757455	284716.038305	52.867981
3201.018613	284531.180520	52.872986
3200.491862	284364.778962	52.877991
3199.688655	284194.397113	52.882996
3199.427821	284014.608050	52.888001
3198.642771	283843.153536	52.893005
3197.930465	283652.102431	52.898010
3197.383658	283490.313467	52.903015
3196.492313	283303.747481	52.908020
3196.231913	283127.090603	52.913025
3195.379489	282955.188009	52.918029
3194.589675	282778.411026	52.923034
3194.286014	282602.499392	52.928039
3193.438620	282417.963594	52.933044
3192.681371	282234.024711	52.938049
3192.068487	282061.650979	52.943053
3191.575747	281883.425959	52.948058
3190.854389	281708.675271	52.953063
3189.922727	281532.939078	52.958068
3189.336340	281341.205070	52.963073
3188.348713	281177.294912	52.968077
3187.898879	281003.927299	52.973082
3187.437919	280819.737380	52.978087
3186.562042	280655.783951	52.983092
3185.962279	280464.841336	52.988097
3185.291763	280293.647807	52.993101
3184.200078	280121.349334	52.998106
3183.905023	279941.258821	53.003111
3183.059880	279774.193213	53.008116
3182.431384	279604.164437	53.013121
3181.851034	279442.354284	53.018125
3181.197564	279259.213205	53.023130
3180.917869	279081.030217	53.028135
3180.189432	278907.044070	53.033140
3179.411576	278733.702423	53.038145
3179.091812	278556.468018	53.043149
3177.874692	278383.679718	53.048154
3177.330327	278209.537001	53.053159
3176.548637	278031.968114	53.058164
3176.261601	277855.492485	53.063169
3175.112383	277686.819229	53.068173
3174.698905	277502.493839	53.073178
3174.155470	277326.338871	53.078183
3173.086208	277148.535234	53.083188
3172.849653	276977.374419	53.088193
3172.249977	276802.145166	53.093197
3171.093991	276626.800174	53.098202
3170.364513	276447.567429	53.103207
3169.797005	276285.270994	53.108212
3169.422582	276105.345344	53.113217
3168.641988	275936.893790	53.118221
3167.816406	275768.041855	53.123226
3167.205981	275596.558097	53.128231
3166.474098	275428.557254	53.133236
3165.793960	275258.281536	53.138241
3165.283339	275080.287540	53.143245
3164.610827	274908.533447	53.148250
3163.802733	274735.247236	53.153255
3163.031055	274580.394383	53.158260
3162.744751	274390.292886	53.163265
3161.816275	274222.654249	53.168269
3161.298461	274049.296660	53.173274
3160.845522	273884.588066	53.178279
3160.150367	273710.698248	53.183284
3159.438735	273535.359351	53.188289
3158.527835	273364.407089	53.193293
3157.951705	273191.364399	53.198298
3157.145977	273020.853953	53.203303
3156.354608	272856.275383	53.208308
3156.470635	272678.105950	53.213313
3155.014085	272512.410181	53.218317
3154.543439	272343.120202	53.223322
3153.913452	272174.339353	53.228327
3153.113300	271999.829601	53.233332
3152.430324	271827.058647	53.238337
3151.412835	271669.239637	53.243341
3151.089354	271488.975089	53.248346
3150.737289	271317.425269	53.253351
3149.639149	271157.912712	53.258356
3149.180389	270977.567782	53.263361
3148.271312	270817.184910	53.268365
3147.679664	270647.608706	53.273370
3147.433404	270481.823600	53.278375
3146.855204	270319.554740	53.283380
3146.195803	270140.056710	53.288385
3145.054630	269975.992343	53.293389
3144.592337	269806.064752	53.298394
3143.684099	269640.690182	53.303399
3142.914013	269476.083306	53.308404
3142.561231	269310.697325	53.313409
3141.875013	269142.307949	53.318413
3140.795377	268980.042316	53.323418
3140.571404	268801.901938	53.328423
3139.927691	268642.088770	53.333428
3139.380971	268473.066255	53.338433
3138.513773	268314.128987	53.343437
3137.770269	268133.829802	53.348442
3137.431198	267967.194055	53.353447
3136.376714	267820.969738	53.358452
3136.059032	267638.285721	53.363457
3135.315627	267464.150044	53.368461
3134.828739	267295.704179	53.373466
3134.136001	267128.462478	53.378471
3133.446801	266961.525891	53.383476
3132.708151	266790.904298	53.388481
3132.049298	266623.912087	53.393485
3131.257279	266460.582952	53.398490
3130.649837	266292.436654	53.403495
3130.317205	266129.289624	53.408500
3129.709133	265951.414722	53.413505
3128.707539	265774.213396	53.418509
3128.154378	265603.715700	53.423514
3127.403786	265433.631335	53.428519
3126.567619	265271.837709	53.433524
3126.231529	265086.279700	53.438529
3125.295023	264929.366491	53.443533
3124.535687	264758.723492	53.448538
3124.078543	264587.421514	53.453543
3123.144278	264426.509668	53.458548
3122.349394	264265.728641	53.463553
3121.632949	264093.016241	53.468557
3121.145998	263937.967867	53.473562
3120.402407	263766.151296	53.478567
3119.696296	263602.325822	53.483572
3119.197183	263441.192740	53.488577
3118.420803	263272.539625	53.493581
3117.799004	263104.244151	53.498586
3117.442089	262951.544153	53.503591
3116.740580	262787.692871	53.508596
3116.051711	262613.499699	53.513601
3115.200697	262447.914959	53.518605
3114.500809	262280.370830	53.523610
3113.950792	262115.910153	53.528615
3112.930670	261955.038518	53.533620
3112.609385	261786.110412	53.538625
3111.904727	261625.189029	53.543629
3110.577361	261462.023234	53.548634
3110.822109	261303.880580	53.553639
3109.652969	261145.605206	53.558644
3109.237040	260979.239312	53.563649
3108.320375	260818.250047	53.568653
3107.790156	260646.477800	53.573658
3107.367045	260484.086298	53.578663
3106.517181	260333.834120	53.583668
3106.377945	260166.406210	53.588673
3105.575563	260002.699755	53.593677
3104.692714	259831.391302	53.598682
3104.184581	259667.052731	53.603687
3103.244204	259507.468710	53.608692
3102.593184	259329.502311	53.613697
3101.956996	259167.425469	53.618701
3101.447539	259000.082353	53.623706
3100.795351	258830.189710	53.628711
3099.754403	258672.124713	53.633716
3099.582882	258499.558539	53.638721
3098.499155	258338.418954	53.643725
3097.764479	258178.472145	53.648730
3097.207952	258018.344446	53.653735
3096.511204	257861.931826	53.658740
3095.783334	257695.464593	53.663745
3095.105102	257539.303933	53.668749
3094.887896	257378.129740	53.673754
3094.240202	257213.432884	53.678759
3093.411884	257054.571293	53.683764
3092.795002	256884.699922	53.688769
3091.933054	256720.852287	53.693773
3091.226667	256559.603289	53.698778
3090.739049	256395.085441	53.703783
3090.000115	256244.181551	53.708788
3089.518724	256072.124646	53.713793
3088.786718	255911.364062	53.718797
3087.894717	255735.883398	53.723802
3086.711492	255583.573189	53.728807
3086.061586	255432.986859	53.733812
3085.944889	255270.448556	53.738817
3085.243463	255111.797523	53.743821
3084.377279	254955.082722	53.748826
3084.053119	254785.625111	53.753831
3083.270836	254628.795418	53.758836
3082.755757	254471.363285	53.763841
3082.136729	254313.005448	53.768845
3081.614871	254145.107694	53.773850
3080.991332	253991.080226	53.778855
3080.175763	253829.392243	53.783860
3079.732290	253657.789795	53.788865
3078.804897	253495.177515	53.793869
3078.238486	253327.542197	53.798874
3077.739408	253160.991450	53.803879
3076.886325	252998.342375	53.808884
3076.051875	252835.130223	53.813889
3075.466415	252672.490015	53.818893
3074.785191	252505.332018	53.823898
3074.273654	252341.967337	53.828903
3073.220368	252192.262324	53.833908
3073.036307	252005.467644	53.838913
3072.146316	251852.273600	53.843917
3071.188268	251694.710191	53.848922
3070.895693	251528.382940	53.853927
3070.264767	251377.465779	53.858932
3069.574088	251199.538131	53.863937
3068.593054	251040.374563	53.868941
3067.502814	250885.761475	53.873946
3067.320144	250720.767345	53.878951
3066.239096	250569.845742	53.883956
3065.653035	250405.679762	53.888961
3065.202846	250252.519420	53.893965
3064.376580	250099.036745	53.898970
3063.807887	249945.029587	53.903975
3063.285316	249783.375358	53.908980
3062.796039	249629.737928	53.913985
3061.961779	249465.764976	53.918989
3061.109214	249304.392654	53.923994
3060.676597	249147.894494	53.928999
3059.921790	248998.705369	53.934004
3059.320864	248831.971257	53.939009
3058.722257	248679.956428	53.944013
3057.738720	248531.007683	53.949018
3057.053488	248369.457050	53.954023
3056.731318	248218.493973	53.959028
3056.137497	248055.477636	53.964033
3055.142801	247903.984660	53.969037
3054.485757	247741.233331	53.974042
3054.309860	247579.220942	53.979047
3053.391602	247429.473507	53.984052
3052.524421	247268.971497	53.989057
3052.106382	247115.579976	53.994061
3051.419449	246947.231745	53.999066
3050.940935	246784.911606	54.004071
3049.918022	246639.154227	54.009076
3049.655976	246463.125021	54.014081
3049.067689	246307.494845	54.019085
3048.179795	246157.056348	54.024090
3047.579131	245984.366416	54.029095
3046.703041	245842.457414	54.034100
3046.139997	245670.602284	54.039105
3045.269129	245506.970565	54.044109
3044.403489	245349.882880	54.049114
3043.728848	245203.206043	54.054119
3043.297784	245043.834420	54.059124
3042.857133	244878.250908	54.064129
3041.777003	244738.845502	54.069133
3041.202901	244586.296352	54.074138
3041.208754	244421.712282	54.079143
3040.014204	244267.148066	54.084148
3039.379884	244105.925288	54.089153
3038.649648	243951.771794	54.094157
3038.426407	243789.898636	54.099162
3037.836396	243636.971121	54.104167
3036.856468	243475.905683	54.109172
3036.342451	243306.515965	54.114177
3035.589076	243149.744169	54.119181
3034.763565	242994.180846	54.124186
3034.309402	242833.414977	54.129191
3033.337546	242688.443229	54.134196
3032.747923	242529.940119	54.139201
3032.143688	242363.418030	54.144205
3031.652530	242212.844833	54.149210
3031.133896	242058.660138	54.154215
3030.061142	241891.270636	54.159220
3029.881431	241728.832995	54.164225
3029.007820	241568.287943	54.169229
3028.179498	241417.056071	54.174234
3027.854206	241251.484467	54.179239
3026.656016	241101.381057	54.184244
3026.110515	240944.579153	54.189249
3025.391117	240787.957769	54.194253
3024.832578	240631.438454	54.199258
3024.435311	240475.021142	54.204263
3023.134207	240318.772564	54.209268
3023.004177	240153.349835	54.214273
3022.194299	240001.887664	54.219277
3021.018887	239848.777426	54.224282
3020.827183	239688.203379	54.229287
3020.246312	239549.845225	54.234292
3019.543797	239384.666996	54.239297
3018.884888	239225.058803	54.244301
3018.316766	239077.455635	54.249306
3017.726030	238910.707076	54.254311
3016.837280	238755.643108	54.259316
3016.338013	238589.186119	54.264321
3015.414487	238425.877700	54.269325
3014.613186	238276.580929	54.274330
3014.077199	238125.561731	54.279335
3012.999338	237975.570682	54.284340
3012.704630	237816.517991	54.289345
3011.899625	237667.833769	54.294349
3011.218690	237518.417120	54.299354
3010.688814	237355.022521	54.304359
3009.637971	237213.151247	54.309364
3009.413171	237068.832194	54.314369
3008.596927	236913.963066	54.319373
3007.561738	236769.136096	54.324378
3007.318323	236615.959195	54.329383
3006.545834	236477.125956	54.334388
3005.940897	236317.538922	54.339393
3005.398525	236176.887195	54.344397
3004.715902	236029.459066	54.349402
3004.006201	235871.544431	54.354407
3003.120999	235716.917151	54.359412
3002.839827	235565.046403	54.364417
3001.938052	235421.091404	54.369421
3001.067118	235273.770550	54.374426
3000.674035	235123.089488	54.379431
3000.119391	234979.080162	54.384436
2999.762347	234829.717925	54.389441
2998.692760	234675.554282	54.394445
2998.274727	234512.426524	54.399450
2997.797211	234359.009932	54.404455
2996.590513	234223.507763	54.409460
2996.180627	234066.898017	54.414465
2995.687742	233915.419738	54.419469
2994.682945	233759.897709	54.424474
2994.223717	233601.412241	54.429479
2993.561767	233466.741548	54.434484
2992.924479	233306.018538	54.439489
2992.457823	233155.657648	54.444493
2991.393555	232992.278214	54.449498
2990.680972	232847.023842	54.454503
2989.886673	232704.965472	54.459508
2989.487943	232559.763702	54.464513
2988.851390	232404.873043	54.469517
2987.942982	232255.423755	54.474522
2987.586101	232101.482361	54.479527
2986.794674	231957.616802	54.484532
2986.398066	231802.307204	54.489537
2985.678025	231650.180948	54.494541
2985.094840	231500.528597	54.499546
2984.325870	231337.741822	54.504551
2983.234963	231192.218862	54.509556
2983.229833	231037.434197	54.514561
2982.300164	230888.856171	54.519565
2981.188693	230733.686978	54.524570
2981.067121	230589.488333	54.529575
2979.869666	230437.719726	54.534580
2979.398779	230293.856928	54.539585
2979.000646	230143.413620	54.544589
2978.242542	229992.492842	54.549594
2977.572878	229833.843328	54.554599
2976.835443	229689.310749	54.559604
2976.069350	229533.554232	54.564609
2975.494243	229393.095802	54.569613
2974.825072	229242.518673	54.574618
2974.456714	229095.356983	54.579623
2973.669912	228950.273256	54.584628
2972.735607	228784.334519	54.589633
2972.027859	228645.120434	54.594637
2971.247489	228500.367433	54.599642
2970.863168	228349.772196	54.604647
2969.957429	228208.425915	54.609652
2969.243522	228062.237273	54.614657
2968.567091	227917.061404	54.619661
2968.049153	227776.723817	54.624666
2967.391364	227628.439190	54.629671
2966.744432	227490.719549	54.634676
2966.381916	227344.170963	54.639681
2965.533940	227193.243762	54.644685
2964.955393	227048.028407	54.649690
2964.311263	226892.893834	54.654695
2963.469134	226750.088603	54.659700
2962.641209	226610.896836	54.664705
2962.292392	226450.522270	54.669709
2961.666352	226303.176990	54.674714
2961.058817	226159.202613	54.679719
2960.347372	226012.507890	54.684724
2959.267829	225859.519222	54.689729
2958.703020	225727.454500	54.694733
2957.883342	225582.725424	54.699738
2957.814516	225427.757105	54.704743
2956.698409	225293.145174	54.709748
2956.307108	225142.531297	54.714753
2955.791458	224991.275408	54.719757
2954.675328	224851.075617	54.724762
2954.636701	224699.973897	54.729767
2953.335069	224552.573216	54.734772
2952.879172	224403.129386	54.739777
2952.029988	224259.833116	54.744781
2951.717587	224122.218878	54.749786
2951.161681	223967.928776	54.754791
2950.314081	223822.252507	54.759796
2949.586050	223675.666470	54.764801
2949.101304	223526.623479	54.769805
2948.391823	223385.228904	54.774810
2947.561641	223233.287788	54.779815
2946.823211	223093.693250	54.784820
2946.486593	222938.784860	54.789825
2945.537298	222795.888988	54.794829
2944.856884	222651.308652	54.799834
2944.197615	222506.725238	54.804839
2943.415004	222369.417641	54.809844
2943.040423	222220.550646	54.814849
2942.571529	222070.769593	54.819853
2941.763595	221922.862868	54.824858
2941.285300	221769.748686	54.829863
2940.033556	221629.245135	54.834868
2939.366687	221478.007205	54.839873
2938.839556	221334.219780	54.844877
2937.809775	221196.558799	54.849882
2937.288774	221050.403224	54.854887
2936.905286	220918.203284	54.859892
2936.044478	220778.250442	54.864897
2935.599317	220632.745611	54.869901
2934.574232	220485.499821	54.874906
2934.132678	220350.866001	54.879911
2933.189426	220215.917238	54.884916
2932.966075	220070.314740	54.889921
2932.303629	219928.766363	54.894925
2931.515339	219800.184009	54.899930
2930.992439	219648.786957	54.904935
2929.867872	219509.158314	54.909940
2929.488952	219358.146406	54.914945
2928.638720	219226.112481	54.919949
2927.928122	219080.321768	54.924954
2927.606265	218944.589577	54.929959
2926.706977	218820.341746	54.934964
2926.129259	218670.406538	54.939969
2925.705392	218532.259987	54.944973
2924.502287	218397.419368	54.949978
2924.022790	218246.871219	54.954983
2923.431246	218119.788188	54.959988
2923.065580	217984.522989	54.964993
2922.556894	217836.767999	54.969997
2921.639564	217690.936456	54.975002
2921.235278	217543.241921	54.980007
2920.525405	217398.307354	54.985012
2919.758572	217259.937527	54.990017
2919.305543	217117.037696	54.995021
2918.406261	216970.899288	55.000026
2917.730516	216818.234053	55.005031
2916.787481	216681.267986	55.010036
2916.521929	216536.252121	55.015041
2915.746165	216400.151143	55.020045
2914.970418	216260.893686	55.025050
2914.625912	216107.426566	55.030055
2913.431434	215973.492968	55.035060
2912.717860	215826.703854	55.040065
2912.436756	215687.687456	55.045069
2911.527047	215557.426360	55.050074
2911.130618	215412.955451	55.055079
2910.602035	215262.154191	55.060084
2909.714645	215116.934282	55.065089
2909.132326	214984.776800	55.070093
2908.360500	214835.249671	55.075098
2908.221789	214693.972532	55.080103
2907.246013	214557.130448	55.085108
2906.502951	214402.966555	55.090113
2905.954166	214255.811075	55.095117
2904.877404	214113.792688	55.100122
2904.525969	213966.479313	55.105127
2903.687642	213833.002693	55.110132
2903.181184	213686.401813	55.115137
2902.505631	213558.067670	55.120141
2901.531885	213415.079842	55.125146
2901.030278	213263.655118	55.130151
2900.383571	213130.556878	55.135156
2899.652354	212989.275338	55.140161
2898.897628	212843.441146	55.145165
2898.294880	212713.442462	55.150170
2897.829454	212561.211757	55.155175
2897.212308	212431.063177	55.160180
2896.888625	212285.060159	55.165185
2895.872333	212151.360574	55.170189
2894.852450	212004.908387	55.175194
2894.765274	211864.685560	55.180199
2893.640949	211725.200013	55.185204
2893.121733	211584.817100	55.190209
2892.879307	211437.504885	55.195213
2891.780405	211292.797824	55.200218
2891.103381	211156.119186	55.205223
2890.134999	211014.561318	55.210228
2889.589747	210872.847673	55.215233
2889.302040	210732.009962	55.220237
2888.432347	210594.115722	55.225242
2888.047325	210450.697593	55.230247
2887.204294	210320.130875	55.235252
2886.633107	210181.324792	55.240257
2885.780319	210037.307107	55.245261
2884.707513	209893.960969	55.250266
2884.284842	209756.761440	55.255271
2883.513790	209620.750124	55.260276
2883.137495	209483.594762	55.265281
2882.511636	209354.841159	55.270285
2881.521338	209217.719970	55.275290
2881.328547	209069.947247	55.280295
2880.041338	208932.008242	55.285300
2879.652820	208802.721841	55.290305
2879.205446	208656.530428	55.295309
2878.645810	208524.764426	55.300314
2878.102153	208383.858006	55.305319
2877.029938	208248.508313	55.310324
2876.119083	208104.071605	55.315329
2875.601625	207965.541989	55.320333
2874.811965	207837.097507	55.325338
2874.235019	207702.090604	55.330343
2873.270784	207582.074202	55.335348
2872.861745	207443.744974	55.340353
2872.441734	207315.764877	55.345357
2871.626203	207171.315303	55.350362
2871.033408	207037.750551	55.355367
2870.126307	206904.643127	55.360372
2869.684384	206779.123946	55.365377
2869.349184	206640.033991	55.370381
2868.582906	206505.097943	55.375386
2867.771527	206358.791556	55.380391
2867.174518	206225.992900	55.385396
2866.487319	206088.003574	55.390401
2865.857344	205957.463380	55.395405
2865.131331	205812.392049	55.400410
2864.431581	205672.725757	55.405415
2863.340404	205544.321234	55.410420
2863.140011	205408.127236	55.415425
2862.707303	205274.337488	55.420429
2861.799670	205149.035511	55.425434
2860.971508	204999.986227	55.430439
2860.586256	204876.523826	55.435444
2860.018746	204731.722789	55.440449
2859.375990	204601.773066	55.445453
2858.378798	204470.365317	55.450458
2858.002937	204324.529566	55.455463
2857.089687	204198.377869	55.460468
2856.482361	204050.543248	55.465473
2856.227626	203919.515515	55.470477
2855.179435	203779.438088	55.475482
2854.777436	203635.568072	55.480487
2854.112777	203495.545145	55.485492
2853.165177	203364.373879	55.490497
2852.744205	203230.434306	55.495501
2851.846469	203083.348117	55.500506
2851.271232	202942.790624	55.505511
2850.442079	202816.692302	55.510516
2849.978074	202681.450061	55.515521
2849.601889	202542.427346	55.520525
2848.454858	202413.504192	55.525530
2848.111456	202271.257289	55.530535
2847.429844	202131.876728	55.535540
2846.716391	201992.425201	55.540545
2845.880484	201857.154762	55.545549
2845.373939	201715.482321	55.550554
2845.052254	201583.019875	55.555559
2844.162076	201449.044328	55.560564
2843.639457	201308.520788	55.565569
2843.005888	201169.809496	55.570573
2842.039396	201030.998566	55.575578
2841.506369	200889.943265	55.580583
2840.537488	200757.279875	55.585588
2839.896169	200619.042047	55.590593
2839.154436	200482.347532	55.595597
2838.429400	200349.226575	55.600602
2838.188151	200219.172519	55.605607
2836.837034	200078.350669	55.610612
2836.314386	199939.803086	55.615617
2835.993232	199810.971572	55.620621
2835.152386	199692.084794	55.625626
2834.501957	199555.772637	55.630631
2833.956714	199422.612759	55.635636
2833.377889	199278.845682	55.640641
2832.773738	199150.238715	55.645645
2832.066779	199019.281456	55.650650
2831.555746	198881.994545	55.655655
2830.574536	198749.936113	55.660660
2829.710687	198611.369634	55.665665
2829.341035	198470.714697	55.670669
2828.488170	198341.245588	55.675674
2828.149446	198205.816434	55.680679
2827.245820	198085.505247	55.685684
2826.839397	197954.146716	55.690689
2825.919906	197821.495476	55.695693
2825.268901	197687.389592	55.700698
2824.903368	197541.773779	55.705703
2823.997059	197411.132007	55.710708
2823.353894	197285.869634	55.715713
2822.843412	197144.044408	55.720717
2821.800993	197011.974570	55.725722
2821.542684	196876.459754	55.730727
2820.844146	196741.002284	55.735732
2820.000091	196606.433485	55.740737
2819.222653	196466.306577	55.745741
2818.311406	196347.603889	55.750746
2817.943470	196212.566251	55.755751
2817.567730	196080.571347	55.760756
2816.845768	195954.917479	55.765761
2816.054868	195816.397746	55.770765
2815.253677	195695.986785	55.775770
2814.971560	195542.614229	55.780775
2813.944776	195423.346653	55.785780
2813.652381	195287.434229	55.790785
2812.836119	195142.201925	55.795789
2812.239420	195013.133163	55.800794
2811.960827	194868.236388	55.805799
2810.930516	194736.157754	55.810804
2810.173901	194606.606385	55.815809
2809.769375	194472.469822	55.820813
2808.901274	194335.556850	55.825818
2808.581609	194190.795759	55.830823
2807.425444	194058.102631	55.835828
2806.611551	193926.284494	55.840833
2806.125746	193791.730003	55.845837
2804.999722	193669.237691	55.850842
2804.701554	193537.720615	55.855847
2804.167662	193403.263851	55.860852
2803.648594	193266.425760	55.865857
2803.154585	193133.655666	55.870861
2802.295004	193000.218574	55.875866
2801.660036	192857.699752	55.880871
2801.056725	192733.091177	55.885876
2800.405029	192593.972970	55.890881
2799.554012	192463.271540	55.895885
2798.722484	192321.243444	55.900890
2798.675087	192179.918597	55.905895
2797.708826	192051.335887	55.910900
2796.967555	191930.657289	55.915905
2796.150249	191788.437631	55.920909
2795.490935	191648.356332	55.925914
2795.052247	191510.861493	55.930919
2794.170969	191385.295223	55.935924
2793.573500	191246.248593	55.940929
2793.029705	191108.059037	55.945933
2792.365051	190980.487410	55.950938
2791.782400	190838.449659	55.955943
2791.226546	190708.507740	55.960948
2790.750903	190572.459123	55.965953
2789.895822	190429.829569	55.970957
2789.277819	190293.702501	55.975962
2788.209723	190158.321422	55.980967
2787.550881	190028.257699	55.985972
2787.123779	189898.348469	55.990977
2786.557151	189759.046788	55.995981
2785.742180	189634.098002	56.000986
2785.200900	189480.238232	56.005991
2784.327820	189354.904976	56.010996
2783.370417	189224.992513	56.016001
2783.215931	189087.256028	56.021005
2782.259273	188955.601181	56.026010
2781.662199	188816.052635	56.031015
2780.914189	188695.701293	56.036020
2780.392376	188551.268872	56.041025
2779.859361	188423.187054	56.046029
2779.112962	188289.121665	56.051034
2778.763411	188152.780105	56.056039
2778.480241	188013.082445	56.061044
2777.586953	187874.537788	56.066049
2776.744680	187734.598732	56.071053
2776.088509	187593.689175	56.076058
2775.529917	187452.332033	56.081063
2774.556836	187323.076153	56.086068
2773.847848	187185.064136	56.091073
2773.555763	187041.961266	56.096077
2772.635803	186913.779494	56.101082
2772.039783	186764.555419	56.106087
2771.246640	186636.163502	56.111092
2770.542068	186494.628857	56.116097
2770.449357	186349.880868	56.121101
2769.457534	186216.470993	56.126106
2768.751826	186065.383723	56.131111
2767.937104	185944.006893	56.136116
2767.676132	185800.826626	56.141121
2767.013315	185661.285261	56.146125
2765.951193	185523.423222	56.151130
2765.278895	185376.938191	56.156135
2764.555968	185236.300868	56.161140
2764.014182	185109.705343	56.166145
2763.190772	184971.438248	56.171149
2762.653243	184847.183545	56.176154
2762.281482	184696.912994	56.181159
2761.278413	184568.102189	56.186164
2760.794123	184422.773565	56.191169
2760.449537	184289.037862	56.196173
2759.539376	184151.804733	56.201178
2758.838108	184019.169477	56.206183
2758.173475	183880.575280	56.211188
2757.519090	183730.848858	56.216193
2756.921187	183592.753833	56.221197
2755.984462	183456.303041	56.226202
2755.384763	183317.178748	56.231207
2754.671451	183185.896314	56.236212
2753.747608	183043.122406	56.241217
2753.491247	182897.406464	56.246221
2752.863682	182772.930098	56.251226
2752.118945	182627.203358	56.256231
2751.601088	182494.543609	56.261236
2750.708304	182349.897065	56.266241
2750.052209	182222.895339	56.271245
2749.268587	182085.317833	56.276250
2748.707579	181942.808043	56.281255
2747.895979	181815.654041	56.286260
2747.397648	181681.657995	56.291265
2746.757260	181540.917531	56.296269
2745.786109	181418.496564	56.301274
2745.127957	181273.333043	56.306279
2744.515962	181147.281499	56.311284
2743.891908	181012.544205	56.316289
2743.331025	180876.156398	56.321293
2742.541830	180753.988335	56.326298
2742.064257	180609.269090	56.331303
2741.308425	180482.339131	56.336308
2740.737448	180360.010418	56.341313
2740.117689	180215.035176	56.346317
2739.342354	180083.186785	56.351322
2738.790797	179948.377737	56.356327
2737.964995	179808.359178	56.361332
2737.209651	179672.578397	56.366337
2736.748506	179543.760141	56.371341
2735.886829	179410.464709	56.376346
2735.566614	179270.024396	56.381351
2734.888664	179136.764319	56.386356
2734.349041	179005.225362	56.391361
2733.840033	178859.283202	56.396365
2732.796611	178736.169042	56.401370
2732.334027	178583.224638	56.406375
2731.700055	178451.702348	56.411380
2730.905750	178312.942982	56.416385
2730.164626	178176.376130	56.421389
2729.195657	178043.954215	56.426394
2728.845195	177904.858780	56.431399
2728.352648	177776.648702	56.436404
2727.596850	177647.921063	56.441409
2727.005048	177510.226144	56.446413
2726.453366	177368.175324	56.451418
2726.115633	177227.363022	56.456423
2725.481643	177085.262609	56.461428
2724.461581	176944.419439	56.466433
2724.191858	176803.394295	56.471437
2723.344728	176661.990489	56.476442
2722.660721	176517.953924	56.481447
2721.996255	176387.574969	56.486452
2721.115795	176239.017096	56.491457
2720.638320	176093.664682	56.496461
2719.958793	175955.403760	56.501466
2718.793977	175818.288557	56.506471
2718.271403	175676.709536	56.511476
2718.071936	175538.348536	56.516481
2717.534451	175392.410334	56.521485
2716.598086	175260.271979	56.526490
2716.260098	175111.746730	56.531495
2715.510883	174965.640097	56.536500
2714.534730	174833.000691	56.541505
2714.222913	174687.461696	56.546509
2713.326843	174541.328981	56.551514
2712.698674	174385.501106	56.556519
2712.002875	174253.785783	56.561524
2711.225585	174106.376710	56.566529
2710.828310	173968.090549	56.571533
2709.960505	173826.814314	56.576538
2709.496303	173680.234761	56.581543
2708.623544	173541.465791	56.586548
2707.728814	173404.023462	56.591553
2707.198198	173264.679811	56.596557
2706.844383	173132.659630	56.601562
2706.197620	172974.970630	56.606567
2705.440849	172844.172570	56.611572
2705.024246	172686.308355	56.616577
2704.508573	172549.419380	56.621581
2703.599635	172409.731682	56.626586
2702.958920	172256.699270	56.631591
2702.425190	172106.435667	56.636596
2701.694317	171967.153724	56.641601
2700.941388	171824.938011	56.646605
2700.166187	171682.624598	56.651610
2699.821234	171537.839941	56.656615
2698.655804	171396.937433	56.661620
2698.127907	171249.779226	56.666625
2697.683888	171100.904162	56.671629
2696.773328	170965.634759	56.676634
2696.152999	170808.725981	56.681639
2695.479431	170667.926222	56.686644
2694.659682	170536.751572	56.691649
2694.032212	170390.680616	56.696653
2693.514106	170241.884152	56.701658
2693.038026	170101.500255	56.706663
2692.015306	169958.838111	56.711668
2691.601812	169817.656877	56.716673
2691.488659	169672.715254	56.721677
2690.450588	169539.543869	56.726682
2690.019576	169386.680233	56.731687
2689.134176	169236.572415	56.736692
2688.253215	169086.642513	56.741697
2687.964418	168945.838935	56.746701
2686.722671	168803.533687	56.751706
2686.356581	168651.985214	56.756711
2685.701380	168511.648208	56.761716
2684.876800	168367.841533	56.766721
2684.860491	168214.700693	56.771725
2683.367838	168063.383897	56.776730
2683.263839	167929.663216	56.781735
2682.448613	167783.619202	56.786740
2681.848133	167631.857597	56.791745
2681.369551	167481.552359	56.796749
2680.777627	167324.983931	56.801754
2680.139163	167180.020543	56.806759
2679.233053	167033.828516	56.811764
2678.386228	166883.685727	56.816769
2677.997336	166724.112103	56.821773
2676.800499	166587.873539	56.826778
2676.370134	166447.902758	56.831783
2675.677057	166295.474556	56.836788
2675.029388	166153.848111	56.841793
2674.496171	166008.656408	56.846797
2674.005054	165864.234251	56.851802
2673.299616	165703.608874	56.856807
2672.392783	165562.979397	56.861812
2671.731307	165424.752945	56.866817
2671.422308	165275.777527	56.871821
2670.579068	165139.717119	56.876826
2669.772626	164982.378708	56.881831
2669.325231	164833.159977	56.886836
2668.458082	164680.079360	56.891841
2668.097122	164533.391184	56.896845
2667.126951	164396.667010	56.901850
2666.536190	164245.972991	56.906855
2666.050135	164101.455197	56.911860
2665.317277	163948.610652	56.916865
2664.992188	163793.337176	56.921869
2664.028021	163644.421299	56.926874
2663.314971	163497.932911	56.931879
2662.663670	163356.902657	56.936884
2662.609011	163199.859659	56.941889
2661.747121	163050.167129	56.946893
2661.091267	162901.637742	56.951898
2660.555577	162732.098280	56.956903
2659.791439	162587.223685	56.961908
2658.649177	162448.156488	56.966913
2658.228964	162282.262586	56.971917
2657.643300	162142.091237	56.976922
2656.936852	161975.633811	56.981927
2656.037154	161828.774893	56.986932
2655.714321	161680.782622	56.991937
2654.892649	161528.509067	56.996941
2654.181953	161381.672892	57.001946
2653.328915	161224.930262	57.006951
2653.080346	161070.330200	57.011956
2652.387135	160923.963551	57.016961
2651.725402	160768.133445	57.021965
2651.008542	160613.749409	57.026970
2650.424337	160464.532214	57.031975
2649.650328	160311.531626	57.036980
2648.984539	160154.980176	57.041985
2648.371400	160001.370615	57.046989
2647.595088	159847.495165	57.051994
2646.821446	159699.607985	57.056999
2646.275885	159535.107059	57.062004
2645.393386	159398.654991	57.067009
2644.795674	159246.139623	57.072013
2644.035051	159094.845770	57.077018
2643.742681	158938.977926	57.082023
2642.749106	158799.799748	57.087028
2642.330293	158654.441511	57.092033
2641.888377	158499.603648	57.097037
2640.846717	158345.586134	57.102042
2640.498165	158195.286061	57.107047
2639.757455	158048.951606	57.112052
2638.922860	157902.022431	57.117057
2638.474654	157732.302330	57.122061
2637.744076	157588.180225	57.127066
2637.168497	157422.867687	57.132071
2636.547310	157279.047354	57.137076
2635.491215	157119.405921	57.142081
2635.419572	156973.109845	57.147085
2634.297927	156811.306402	57.152090
2634.036470	156657.516021	57.157095
2633.248894	156498.928183	57.162100
2632.450508	156350.461699	57.167105
2632.224602	156185.417507	57.172109
2631.115878	156040.421105	57.177114
2630.633204	155874.109756	57.182119
2629.899061	155717.296760	57.187124
2629.316445	155571.481699	57.192129
2628.843697	155410.192246	57.197133
2627.929447	155265.664092	57.202138
2627.135103	155103.613496	57.207143
2626.645994	154956.476952	57.212148
2625.562469	154796.558360	57.217153
2625.275508	154641.980283	57.222157
2624.533445	154502.233078	57.227162
2623.843335	154355.194558	57.232167
2623.089731	154145.868250	57.237172
2622.867887	153965.936488	57.242177
2622.491612	153808.872259	57.247181
2621.533769	153652.790697	57.252186
2621.206722	153482.538700	57.257191
2620.498739	153333.168645	57.262196
2619.667334	153161.574559	57.267201
2618.884250	153004.476878	57.272205
2617.937266	152840.758120	57.277210
2617.256879	152680.302738	57.282215
2616.931931	152526.312428	57.287220
2615.969641	152374.533796	57.292225
2615.801954	152204.034294	57.297229
2614.756153	152060.405141	57.302234
2614.339692	151898.500851	57.307239
2613.653262	151745.982317	57.312244
2612.801129	151588.330324	57.317249
2612.066162	151429.186122	57.322253
2611.382230	151271.026006	57.327258
2610.904201	151114.727846	57.332263
2609.974915	150962.505634	57.337268
2609.284170	150798.400526	57.342273
2609.024165	150650.662056	57.347277
2608.081612	150492.254350	57.352282
2607.566789	150337.859519	57.357287
2607.014892	150163.847290	57.362292
2606.241135	150000.267744	57.367297
2605.773610	149838.114825	57.372301
2604.805372	149691.102997	57.377306
2604.611141	149518.893159	57.382311
2603.696741	149373.005399	57.387316
2602.516135	149210.803389	57.392321
2602.220489	149030.656093	57.397325
2601.341689	148895.999959	57.402330
2600.493623	148734.205190	57.407335
2600.196604	148571.180088	57.412340
2599.402886	148427.895584	57.417345
2599.076882	148265.575630	57.422349
2598.044232	148113.522990	57.427354
2597.891380	147948.165164	57.432359
2597.312961	147801.888156	57.437364
2596.135388	147638.321052	57.442369
2595.934895	147466.860312	57.447373
2594.988511	147315.674710	57.452378
2594.525443	147149.976208	57.457383
2593.817459	146993.975906	57.462388
2592.919410	146834.092264	57.467393
2592.394301	146672.218646	57.472397
2591.633526	146526.078073	57.477402
2590.990493	146353.740341	57.482407
2590.494230	146189.513583	57.487412
2589.463346	146039.910582	57.492417
2589.191996	145877.505207	57.497421
2588.613078	145709.507023	57.502426
2587.710374	145549.223974	57.507431
2587.296794	145389.385262	57.512436
2586.509485	145219.618196	57.517441
2585.957125	145079.042788	57.522445
2584.762229	144909.329288	57.527450
2584.425360	144748.515906	57.532455
2583.804347	144584.215662	57.537460
2583.295564	144430.242447	57.542465
2582.505103	144261.535823	57.547469
2581.741150	144114.047306	57.552474
2580.913524	143959.707605	57.557479
2580.260037	143790.155861	57.562484
2579.749066	143633.886926	57.567489
2579.250037	143473.931812	57.572493
2578.286604	143321.230629	57.577498
2577.888343	143159.533010	57.582503
2577.326027	142993.402093	57.587508
2576.402692	142843.848251	57.592513
2575.819907	142670.542923	57.597517
2575.289788	142518.895259	57.602522
2575.032722	142349.314041	57.607527
2574.272159	142191.757781	57.612532
2573.167618	142028.106866	57.617537
2572.473137	141858.114839	57.622541
2571.919858	141697.122945	57.627546
2571.265500	141537.113603	57.632551
2570.541877	141389.377653	57.637556
2569.775323	141235.308815	57.642561
2569.626979	141063.836993	57.647565
2568.840653	140904.042493	57.652570
2568.175826	140724.230302	57.657575
2567.281560	140579.587493	57.662580
2566.697423	140414.668449	57.667585
2566.503910	140245.266779	57.672589
2565.636942	140082.452716	57.677594
2565.012987	139912.130085	57.682599
2564.390003	139741.592269	57.687604
2563.443925	139573.431738	57.692609
2563.211554	139416.581258	57.697613
2562.288424	139238.711994	57.702618
2561.571602	139075.752550	57.707623
2561.116440	138900.809592	57.712628
2559.910309	138744.752218	57.717633
2559.692842	138572.848170	57.722637
2558.791496	138427.136940	57.727642
2558.289392	138248.825711	57.732647
2557.397127	138084.362195	57.737652
2556.747038	137920.521865	57.742657
2556.320232	137747.105784	57.747661
2555.507454	137598.729299	57.752666
2554.586972	137423.830674	57.757671
2554.147591	137261.967931	57.762676
2553.589231	137108.192276	57.767681
2553.056416	136930.745063	57.772685
2552.104226	136774.492686	57.777690
2551.702909	136610.696435	57.782695
2551.370278	136436.752268	57.787700
2550.317842	136275.881407	57.792705
2549.508990	136100.960264	57.797709
2548.989437	135948.531169	57.802714
2548.343638	135772.633354	57.807719
2547.975622	135610.997087	57.812724
2547.155741	135441.544296	57.817729
2546.658084	135265.346585	57.822733
2545.913231	135106.821725	57.827738
2545.163562	134931.809304	57.832743
2544.647415	134763.608095	57.837748
2543.937330	134587.486280	57.842753
2543.386399	134415.024275	57.847757
2542.534374	134241.734494	57.852762
2541.968215	134077.330770	57.857767
2541.304788	133911.304702	57.862772
2540.708865	133745.052943	57.867777
2540.050892	133563.886031	57.872781
2539.027003	133402.493088	57.877786
2538.474276	133233.417413	57.882791
2537.896171	133063.355947	57.887796
2536.858067	132902.869968	57.892801
2536.505010	132725.521641	57.897805
2535.773961	132575.608180	57.902810
2535.605244	132392.541992	57.907815
2534.514152	132222.223878	57.912820
2533.662777	132053.062807	57.917825
2533.227539	131884.433794	57.922829
2532.520160	131718.097188	57.927834
2532.119756	131541.144817	57.932839
2531.649110	131376.093713	57.937844
2530.613561	131215.578762	57.942849
2529.814478	131035.466465	57.947853
2529.102396	130866.900101	57.952858
2528.334471	130697.187746	57.957863
2527.790385	130539.520139	57.962868
2526.819628	130374.160420	57.967873
2526.776125	130198.595185	57.972877
2525.947160	130048.151796	57.977882
2525.172708	129873.339517	57.982887
2524.738992	129704.964640	57.987892
2523.977970	129534.229440	57.992897
2523.458884	129371.268084	57.997901
2522.409804	129191.931223	58.002906
2522.058014	129027.141830	58.007911
2521.355842	128865.546048	58.012916
2520.460877	128688.093136	58.017921
2519.863629	128518.392379	58.022925
2519.369854	128352.791251	58.027930
2518.835005	128188.708984	58.032935
2517.826952	128011.748253	58.037940
2516.992905	127846.572403	58.042945
2516.675864	127676.108488	58.047949
2515.958992	127523.692478	58.052954
2515.547790	127338.792751	58.057959
2514.505201	127181.655020	58.062964
2513.714977	127013.962617	58.067969
2513.640394	126844.202033	58.072973
2512.786137	126674.642273	58.077978
2511.874954	126511.226559	58.082983
2511.605860	126340.750643	58.087988
2511.082268	126175.319761	58.092993
2510.305785	125990.601335	58.097997
2509.629717	125827.749329	58.103002
2508.706506	125655.057387	58.108007
2508.081203	125474.763272	58.113012
2507.454577	125308.998413	58.118017
2506.980718	125131.463696	58.123021
2506.184038	124963.619857	58.128026
2505.275457	124813.243134	58.133031
2504.928009	124625.697639	58.138036
2504.207035	124468.346832	58.143041
2503.368994	124287.472115	58.148045
2502.957668	124117.235907	58.153050
2502.015849	123942.780059	58.158055
2501.420522	123765.946611	58.163060
2500.315130	123609.030023	58.168065
2500.060191	123432.805136	58.173069
2499.363198	123277.971768	58.178074
2499.020264	123098.017061	58.183079
2498.503692	122947.080737	58.188084
2497.857877	122756.027452	58.193089
2497.431348	122576.318078	58.198093
2496.585084	122416.116777	58.203098
2495.244930	122246.979341	58.208103
2494.987125	122068.237082	58.213108
2494.094355	121900.922891	58.218113
2493.614118	121725.011666	58.223117
2492.914471	121568.004714	58.228122
2492.312817	121383.937880	58.233127
2491.818625	121216.666422	58.238132
2490.963364	121033.239004	58.243137
2490.206673	120866.938265	58.248141
2489.706553	120699.277425	58.253146
2489.074735	120528.400820	58.258151
2488.517720	120348.701884	58.263156
2487.791477	120186.984175	58.268161
2487.637984	120004.798561	58.273165
2486.625134	119840.538307	58.278170
2485.837821	119655.598864	58.283175
2485.238293	119480.889647	58.288180
2484.227011	119318.041735	58.293185
2484.289309	119131.815975	58.298189
2483.160594	118949.163849	58.303194
2482.634420	118788.489576	58.308199
2481.916576	118607.222081	58.313204
2481.348480	118429.353656	58.318209
2480.570551	118255.284014	58.323213
2480.397585	118071.966050	58.328218
2479.522162	117901.075478	58.333223
2478.853158	117724.059464	58.338228
2478.087652	117556.226072	58.343233
2477.309457	117357.565117	58.348237
2476.377374	117198.723380	58.353242
2475.807133	117016.015452	58.358247
2475.151416	116837.048382	58.363252
2474.425569	116676.742643	58.368257
2474.067146	116500.371363	58.373261
2473.169486	116324.454926	58.378266
2472.741986	116150.134534	58.383271
2472.099678	115976.534894	58.388276
2471.271362	115802.572390	58.393281
2471.102809	115623.238281	58.398285
2469.968494	115449.897946	58.403290
2469.265594	115264.887810	58.408295
2468.734648	115084.021816	58.413300
2467.980218	114912.027653	58.418305
2467.288285	114735.448549	58.423309
2466.846356	114558.627945	58.428314
2465.998997	114378.540707	58.433319
2465.738422	114205.381398	58.438324
2464.599720	114028.757467	58.443329
2464.252014	113851.222388	58.448333
2463.187019	113672.437713	58.453338
2462.428560	113500.974250	58.458343
2462.049849	113332.263336	58.463348
2461.291774	113157.102057	58.468353
2460.816038	112977.111927	58.473357
2459.820180	112799.985324	58.478362
2459.658471	112618.456562	58.483367
2458.964134	112447.478835	58.488372
2457.942143	112281.193440	58.493377
2457.506251	112094.038278	58.498381
2456.726196	111925.952620	58.503386
2455.980897	111750.259763	58.508391
2455.285359	111568.626547	58.513396
2454.300661	111398.438228	58.518401
2454.022310	111215.979923	58.523405
2453.065621	111048.416870	58.528410
2452.755546	110878.994598	58.533415
2452.049114	110705.765260	58.538420
2451.347896	110538.406321	58.543425
2450.814203	110358.717244	58.548429
2450.050655	110196.973945	58.553434
2449.240533	110025.726704	58.558439
2449.087780	109844.426272	58.563444
2448.158960	109668.485431	58.568449
2447.359370	109495.691865	58.573453
2446.831936	109322.190083	58.578458
2446.164964	109138.653887	58.583463
2445.630648	108968.081030	58.588468
2444.742674	108785.972195	58.593473
2444.106490	108607.105408	58.598477
2443.582368	108437.994099	58.603482
2442.775457	108260.705204	58.608487
2442.213243	108088.639080	58.613492
2441.257741	107913.800187	58.618497
2440.898601	107743.087592	58.623501
2439.692106	107566.343012	58.628506
2439.235308	107400.978266	58.633511
2439.175151	107224.543035	58.638516
2438.250561	107057.332237	58.643521
2437.847275	106873.454121	58.648525
2436.783700	106692.898975	58.653530
2436.422045	106509.131251	58.658535
2435.676069	106338.432816	58.663540
2435.077453	106162.154178	58.668545
2434.296285	105980.360450	58.673549
2433.238977	105826.014725	58.678554
2432.939078	105637.523414	58.683559
2432.510520	105466.324058	58.688564
2431.697035	105302.248472	58.693569
2431.007370	105113.207664	58.698573
2430.336798	104937.780596	58.703578
2429.481081	104763.906837	58.708583
2429.055880	104590.771839	58.713588
2428.267770	104418.311036	58.718593
2427.590676	104234.027142	58.723597
2427.018899	104070.321431	58.728602
2426.509849	103877.880331	58.733607
2426.129681	103702.835071	58.738612
2425.161462	103529.337134	58.743617
2424.836589	103336.820488	58.748621
2423.997928	103173.448783	58.753626
2423.349864	102982.749902	58.758631
2422.481566	102798.000008	58.763636
2421.520556	102627.387712	58.768641
2420.852944	102446.941627	58.773645
2420.226987	102277.192269	58.778650
2419.847723	102096.436730	58.783655
2419.402261	101914.659061	58.788660
2418.466806	101747.899730	58.793665
2417.745050	101568.211208	58.798669
2417.129471	101393.398100	58.803674
2416.330770	101208.345233	58.808679
2415.860409	101040.553017	58.813684
2415.269221	100870.078883	58.818689
2414.843186	100675.785942	58.823693
2414.165627	100509.850944	58.828698
2413.335377	100331.356342	58.833703
2412.832037	100138.501044	58.838708
2412.213900	99951.349005	58.843713
2411.892968	99772.321261	58.848717
2410.644120	99592.674509	58.853722
2409.869136	99408.659826	58.858727
2409.432972	99242.257991	58.863732
2408.650329	99051.098880	58.868737
2408.262221	98863.177086	58.873741
2406.770478	98688.884860	58.878746
2406.449547	98514.262454	58.883751
2405.931073	98328.756918	58.888756
2405.452509	98160.333641	58.893761
2404.868537	97973.388903	58.898765
2404.148542	97800.554052	58.903770
2403.457734	97607.267675	58.908775
2403.123864	97430.378639	58.913780
2401.971590	97253.392403	58.918785
2401.631969	97059.585657	58.923789
2400.770211	96885.200983	58.928794
2399.887548	96711.233210	58.933799
2399.604136	96522.324690	58.938804
2398.861688	96342.914939	58.943809
2398.319725	96158.039654	58.948813
2397.227646	95980.597179	58.953818
2396.529410	95798.635238	58.958823
2396.348583	95617.524995	58.963828
2395.392463	95447.352044	58.968833
2395.039720	95250.328504	58.973837
2394.118471	95076.113084	58.978842
2393.870086	94903.574361	58.983847
2393.368879	94712.641771	58.988852
2392.433955	94530.404185	58.993857
2391.624119	94341.242272	58.998861
2390.923452	94159.268621	59.003866
2390.411458	93969.694818	59.008871
2389.665360	93785.283606	59.013876
2388.636146	93607.139689	59.018881
2388.107966	93429.602619	59.023885
2387.541038	93256.378829	59.028890
2386.727144	93061.540290	59.033895
2386.267491	92884.611802	59.038900
2385.528939	92710.696583	59.043905
2384.808026	92520.692659	59.048909
2384.209854	92341.685231	59.053914
2383.306204	92149.697023	59.058919
2383.169524	91974.278127	59.063924
2382.083572	91804.660832	59.068929
2381.702012	91616.988687	59.073933
2381.275352	91447.631030	59.078938
2380.103603	91256.098914	59.083943
2379.961785	91059.713093	59.088948
2379.199113	90884.268969	59.093953
2378.383312	90692.419025	59.098957
2377.675487	90510.793513	59.103962
2377.024127	90328.031957	59.108967
2376.583964	90141.649789	59.113972
2375.694922	89967.640605	59.118977
2374.933388	89766.133864	59.123981
2374.370441	89586.363437	59.128986
2373.336794	89408.900862	59.133991
2373.247811	89224.391912	59.138996
2372.459416	89050.481873	59.144001
2371.912015	88864.057887	59.149005
2371.141034	88677.531472	59.154010
2370.452244	88485.896355	59.159015
2369.950972	88295.868878	59.164020
2369.208842	88126.295362	59.169025
2368.484295	87930.714803	59.174029
2367.856731	87753.873395	59.179034
2367.280272	87564.625028	59.184039
2366.492838	87379.323287	59.189044
2366.016617	87191.380933	59.194049
2365.003371	87008.134157	59.199053
2364.436274	86835.360635	59.204058
2363.744397	86641.593331	59.209063
2363.181922	86454.324054	59.214068
2362.266690	86278.275749	59.219073
2361.698869	86089.742658	59.224077
2361.103707	85910.755957	59.229082
2360.746006	85730.826615	59.234087
2360.131365	85545.728849	59.239092
2359.074120	85362.338325	59.244097
2358.715339	85172.803982	59.249101
2357.682699	84983.409870	59.254106
2357.166964	84812.894848	59.259111
2356.732962	84621.691221	59.264116
2355.570214	84440.670716	59.269121
2355.063450	84259.078682	59.274125
2354.379275	84082.492129	59.279130
2353.685417	83909.331394	59.284135
2352.945020	83717.924627	59.289140
2352.437916	83541.244794	59.294145
2351.937105	83356.908688	59.299149
2351.067359	83175.846220	59.304154
2350.621193	82994.990690	59.309159
2350.164550	82800.631657	59.314164
2349.194956	82624.603287	59.319169
2348.572908	82437.081021	59.324173
2348.320080	82253.349074	59.329178
2346.850894	82070.445410	59.334183
2346.716444	81886.761287	59.339188
2345.856998	81707.034487	59.344193
2345.306403	81517.544386	59.349197
2344.783380	81337.539259	59.354202
2343.908675	81154.701457	59.359207
2343.184361	80965.909373	59.364212
2342.307758	80786.592500	59.369217
2341.744928	80605.668385	59.374221
2341.053109	80424.544488	59.379226
2340.713575	80247.834196	59.384231
2340.344054	80065.306117	59.389236
2339.590537	79886.421121	59.394241
2339.047753	79692.649712	59.399245
2338.107580	79510.945796	59.404250
2337.142617	79323.062353	59.409255
2337.002000	79135.626579	59.414260
2335.938968	78962.590765	59.419265
2335.537238	78781.390902	59.424269
2334.835810	78593.637083	59.429274
2334.028630	78402.365779	59.434279
2333.616110	78216.901555	59.439284
2332.690148	78036.862306	59.444289
2332.482495	77852.883370	59.449293
2331.639607	77671.991374	59.454298
2330.887760	77472.545711	59.459303
2330.606552	77277.519952	59.464308
2329.174972	77097.360047	59.469313
2328.953604	76907.302457	59.474317
2328.159391	76718.325947	59.479322
2327.523238	76539.869705	59.484327
2326.969841	76349.153975	59.489332
2325.949795	76176.755868	59.494337
2325.753883	75979.390965	59.499341
2324.856110	75794.241139	59.504346
2324.379685	75610.667213	59.509351
2323.833786	75422.366686	59.514356
2322.986383	75239.045037	59.519361
2322.123197	75050.272413	59.524365
2321.920300	74861.631271	59.529370
2321.107581	74665.777196	59.534375
2320.719882	74477.789849	59.539380
2319.467889	74303.195357	59.544385
2318.975471	74104.520965	59.549389
2318.364547	73914.173122	59.554394
2317.723208	73727.417745	59.559399
2317.054614	73540.091914	59.564404
2316.023841	73346.591348	59.569409
2315.562130	73170.785391	59.574413
2314.806863	72993.570442	59.579418
2314.422995	72809.190169	59.584423
2313.559406	72623.633334	59.589428
2312.676646	72440.887669	59.594433
2312.431661	72249.813458	59.599437
2311.719126	72068.501252	59.604442
2310.794318	71881.998137	59.609447
2310.543346	71690.005369	59.614452
2309.508514	71505.873431	59.619457
2309.041926	71315.008053	59.624461
2308.534353	71136.877182	59.629466
2307.596670	70951.176690	59.634471
2307.085224	70758.930193	59.639476
2305.985418	70572.061762	59.644481
2305.809053	70387.652070	59.649485
2305.211211	70205.097210	59.654490
2304.331811	70022.987750	59.659495
2303.591692	69831.065270	59.664500
2303.026907	69649.682140	59.669505
2302.276235	69456.890882	59.674509
2301.618502	69278.255896	59.679514
2301.362508	69092.040458	59.684519
2300.405968	68901.263496	59.689524
2299.579565	68722.020612	59.694529
2298.830334	68537.706471	59.699533
2298.377348	68353.803113	59.704538
2297.246906	68161.623207	59.709543
2297.427343	67982.740459	59.714548
2296.666691	67797.010075	59.719553
2296.123765	67608.808559	59.724557
2295.374738	67419.849878	59.729562
2294.590165	67231.646003	59.734567
2294.122598	67036.750093	59.739572
2293.257970	66848.017976	59.744577
2292.768122	66664.399266	59.749581
2291.985217	66474.321541	59.754586
2291.134461	66293.337984	59.759591
2290.612636	66104.451096	59.764596
2289.714715	65914.973414	59.769601
2288.965778	65723.447463	59.774605
2288.521363	65532.875697	59.779610
2287.480087	65354.448444	59.784615
2287.184586	65166.931214	59.789620
2286.155788	64993.983066	59.794625
2285.781726	64804.297093	59.799629
2285.493143	64608.805237	59.804634
2284.395858	64426.567523	59.809639
2283.823359	64245.790242	59.814644
2283.173544	64060.958441	59.819649
2282.541518	63872.921506	59.824653
2281.862792	63693.796838	59.829658
2281.095921	63503.913772	59.834663
2280.849175	63310.030582	59.839668
2279.842281	63143.345422	59.844673
2279.320030	62950.820303	59.849677
2278.634167	62764.423816	59.854682
2277.978586	62581.506838	59.859687
2277.623518	62386.833440	59.864692
2276.655160	62209.908808	59.869697
2276.229938	62005.961902	59.874701
2275.234762	61820.336060	59.879706
2274.787792	61631.234595	59.884711
2274.333789	61446.545962	59.889716
2273.341804	61258.611007	59.894721
2272.861629	61065.484245	59.899725
2272.481026	60868.924815	59.904730
2271.403103	60680.661042	59.909735
2270.602467	60487.704995	59.914740
2269.916164	60309.560051	59.919745
2269.453697	60118.988438	59.924750
2268.591034	59931.954731	59.929754
2268.085799	59743.099899	59.934759
2267.519936	59546.786282	59.939764
2266.669963	59364.285900	59.944769
2265.932138	59184.285944	59.949774
2265.474352	58991.648619	59.954778
2264.646032	58811.346920	59.959783
2264.152589	58620.273229	59.964788
2263.528370	58429.956565	59.969793
2263.082108	58240.490373	59.974798
2262.330616	58048.754483	59.979802
2261.630657	57868.270651	59.984807
2260.842794	57664.194294	59.989812
2260.136879	57482.756146	59.994817
2259.685682	57296.417934	59.999822
2258.812343	57109.439599	60.004826
2258.409444	56917.394272	60.009831
2257.827368	56731.987679	60.014836
2256.934636	56544.432634	60.019841
2256.406054	56338.576450	60.024846
2255.669568	56166.650593	60.029850
2255.076153	55970.964670	60.034855
2254.806821	55760.206412	60.039860
2253.728711	55573.741359	60.044865
2253.266307	55378.822645	60.049870
2252.520981	55194.090379	60.054874
2252.018373	55000.758052	60.059879
2251.136064	54800.608212	60.064884
2249.978481	54614.064270	60.069889
2249.521906	54422.832006	60.074894
2248.659509	54238.764027	60.079898
2247.964850	54056.009861	60.084903
2247.233129	53865.709959	60.089908
2246.592917	53686.042497	60.094913
2246.100854	53498.638636	60.099918
2245.661529	53308.779162	60.104922
2244.917605	53125.127676	60.109927
2244.738317	52932.882991	60.114932
2243.933152	52741.476878	60.119937
2243.210114	52542.437252	60.124942
2242.325852	52357.224227	60.129946
2241.569729	52173.356508	60.134951
2241.093658	51968.006433	60.139956
2240.335078	51795.992425	60.144961
2239.615519	51602.961636	60.149966
2238.923702	51402.879169	60.154970
2238.282010	51227.406477	60.159975
2238.058243	51034.505636	60.164980
2237.162348	50862.610918	60.169985
2236.564029	50655.162747	60.174990
2235.730350	50457.093881	60.179994
2234.964490	50274.310155	60.184999
2234.894198	50078.082772	60.190004
2233.869627	49892.607340	60.195009
2233.066996	49688.119722	60.200014
2232.188585	49500.413770	60.205018
2231.983515	49311.685542	60.210023
2231.167179	49125.489059	60.215028
2230.597352	48933.627477	60.220033
2230.107770	48736.342471	60.225038
2229.296018	48543.846476	60.230042
2228.280756	48361.207331	60.235047
2228.007062	48165.937997	60.240052
2227.307087	47975.837784	60.245057
2226.693577	47784.001876	60.250062
2225.721473	47589.713264	60.255066
2225.043252	47397.898133	60.260071
2224.332229	47210.205656	60.265076
2223.295848	47035.279698	60.270081
2223.058512	46846.143124	60.275086
2222.388630	46671.694050	60.280090
2221.388262	46479.073308	60.285095
2221.296596	46297.779829	60.290100
2220.678515	46104.808378	60.295105
2219.756578	45914.518864	60.300110
2219.200420	45722.652004	60.305114
2218.242926	45540.671817	60.310119
2217.801074	45349.217908	60.315124
2217.201212	45172.384628	60.320129
2216.609967	44988.119102	60.325134
2216.221219	44783.654215	60.330138
2214.952028	44600.676875	60.335143
2214.642869	44410.505765	60.340148
2214.111088	44221.709863	60.345153
2213.496029	44030.471826	60.350158
2212.656323	43841.811116	60.355162
2212.010651	43648.890123	60.360167
2211.415949	43449.929026	60.365172
2210.341892	43266.713383	60.370177
2209.647296	43080.507855	60.375182
2209.219115	42887.133892	60.380186
2208.472514	42711.677112	60.385191
2207.738678	42512.517987	60.390196
2207.255913	42326.935250	60.395201
2206.291065	42141.272862	60.400206
2205.579008	41946.600974	60.405210
2205.192663	41771.033355	60.410215
2204.508036	41587.881247	60.415220
2203.498542	41406.218253	60.420225
2203.020158	41224.017577	60.425230
2202.568991	41031.177158	60.430234
2201.859470	40860.172948	60.435239
2201.004445	40664.270251	60.440244
2200.774435	40484.738405	60.445249
2199.888153	40280.642789	60.450254
2199.288824	40107.530635	60.455258
2198.502529	39931.140952	60.460263
2198.208685	39730.964054	60.465268
2197.430342	39542.538287	60.470273
2196.586116	39350.305592	60.475278
2196.112501	39173.418835	60.480282
2195.197858	38984.260453	60.485287
2194.934652	38794.491799	60.490292
2194.159066	38602.549113	60.495297
2193.222501	38406.051350	60.500302
2192.607270	38222.133872	60.505306
2191.716509	38034.917165	60.510311
2191.207170	37854.132631	60.515316
2190.648404	37665.836677	60.520321
2189.722964	37475.628238	60.525326
2189.650748	37292.417169	60.530330
2188.820567	37112.086637	60.535335
2188.407561	36923.331653	60.540340
2187.550013	36735.788956	60.545345
2187.213841	36537.377764	60.550350
2186.256102	36342.465849	60.555354
2185.337603	36166.768534	60.560359
2185.043514	35964.537095	60.565364
2184.048867	35779.380298	60.570369
2183.229519	35599.555805	60.575374
2182.878088	35406.186536	60.580378
2181.947224	35220.553212	60.585383
2181.517897	35030.355347	60.590388
2180.603594	34847.737540	60.595393
2179.992623	34650.613952	60.600398
2179.336478	34467.009493	60.605402
2178.545149	34290.355514	60.610407
2178.420993	34096.604989	60.615412
2177.383328	33921.789341	60.620417
2176.797788	33724.241216	60.625422
2176.370148	33535.267523	60.630426
2175.600367	33345.975715	60.635431
2175.225269	33155.427147	60.640436
2173.904806	32967.203657	60.645441
2173.433347	32785.345748	60.650446
2173.210297	32587.897435	60.655450
2172.344538	32412.981906	60.660455
2171.607978	32208.353597	60.665460
2170.978738	32022.140802	60.670465
2170.427982	31825.003253	60.675470
2169.747259	31646.898190	60.680474
2169.204844	31458.979283	60.685479
2168.449905	31263.506820	60.690484
2167.814216	31078.358074	60.695489
2167.296952	30886.052134	60.700494
2166.455136	30693.656145	60.705498
2165.706038	30503.096377	60.710503
2165.293577	30309.925737	60.715508
2164.649467	30125.082958	60.720513
2163.588984	29920.750938	60.725518
2162.955065	29736.086314	60.730522
2161.940981	29546.360228	60.735527
2161.639597	29364.669532	60.740532
2160.760344	29174.763635	60.745537
2160.115976	28994.722466	60.750542
2159.452012	28808.180351	60.755546
2158.723700	28628.019099	60.760551
2158.267553	28433.057537	60.765556
2157.612811	28248.787476	60.770561
2156.861436	28067.391168	60.775566
2156.179418	27879.524445	60.780570
2155.430358	27687.147581	60.785575
2154.771083	27506.027297	60.790580
2154.031022	27318.752896	60.795585
2153.253812	27144.084987	60.800590
2152.744817	26949.978197	60.805594
2152.166435	26782.370075	60.810599
2151.309331	26584.611381	60.815604
2150.798067	26417.048530	60.820609
2149.741636	26222.383352	60.825614
2149.810397	26050.960072	60.830618
2148.799388	25858.635469	60.835623
2148.011482	25678.390122	60.840628
2147.410915	25505.744077	60.845633
2147.129280	25310.432312	60.850638
2146.344212	25130.275588	60.855642
2145.360919	24952.793304	60.860647
2144.859924	24758.484199	60.865652
2144.307325	24578.712988	60.870657
2143.579385	24393.156789	60.875662
2142.987958	24217.311307	60.880666
2141.904775	24027.725714	60.885671
2141.424951	23840.679532	60.890676
2140.595111	23668.515315	60.895681
2139.875284	23481.312419	60.900686
2139.345904	23314.453720	60.905690
2138.609739	23137.042419	60.910695
2138.347219	22945.886485	60.915700
2137.266258	22777.964065	60.920705
2136.615325	22589.372513	60.925710
2136.070853	22421.069471	60.930714
2135.319903	22237.391357	60.935719
2134.830015	22055.035254	60.940724
2133.661449	21885.116339	60.945729
2133.392441	21711.302750	60.950734
2132.805927	21529.350199	60.955738
2132.006892	21350.548371	60.960743
2131.519641	21176.701852	60.965748
2130.666524	20996.244242	60.970753
2129.664888	20826.800544	60.975758
2128.753328	20662.532512	60.980762
2127.979954	20487.324904	60.985767
2127.903248	20308.570689	60.990772
2127.290379	20151.623778	60.995777
2126.622513	19974.433302	61.000782
2126.009403	19794.776033	61.005786
2125.203364	19625.415299	61.010791
2124.738677	19451.748069	61.015796
2123.533625	19282.364349	61.020801
2123.011716	19116.169724	61.025806
2122.398920	18934.196479	61.030810
2121.560406	18774.148801	61.035815
2121.133077	18603.178675	61.040820
2119.943013	18446.707906	61.045825
2119.511461	18279.027249	61.050830
2118.883218	18114.251518	61.055834
2118.052244	17947.810877	61.060839
2117.248485	17800.664326	61.065844
2116.442118	17629.402675	61.070849
2116.236949	17471.870907	61.075854
2115.449942	17299.986193	61.080858
2114.414731	17157.914356	61.085863
2113.675090	17000.379222	61.090868
2112.647783	16839.492555	61.095873
2112.254475	16684.413069	61.100878
2111.584381	16538.193634	61.105882
2110.709772	16386.167151	61.110887
2110.492127	16229.468311	61.115892
2109.596055	16088.763548	61.120897
2108.863493	15933.030490	61.125902
2108.123920	15789.174596	61.130906
2107.077832	15649.957254	61.135911
2106.666897	15500.407249	61.140916
2105.528494	15366.327433	61.145921
2104.896832	15233.682405	61.150926
2103.831799	15095.137947	61.155930
2102.904652	14976.017606	61.160935
2102.009846	14840.344631	61.165940
2101.071619	14732.417904	61.170945
2100.220063	14614.828983	61.175950
2099.417025	14506.705502	61.180954
2098.381510	14420.826427	61.185959
2097.506727	14320.367959	61.190964
2096.560773	14229.814164	61.195969
2095.259001	14135.054719	61.200974
2094.408317	14049.889868	61.205978
2093.655267	13972.130945	61.210983
2092.927412	13894.879036	61.215988
2092.023915	13830.497597	61.220993
2091.197649	13752.658676	61.225998
2090.541542	13700.833073	61.231002
2089.574821	13627.475252	61.236007
2089.397041	13557.040935	61.241012
2088.299720	13503.177301	61.246017
2087.658199	13438.005529	61.251022
2087.463330	13372.259565	61.256026
2086.436956	13315.093743	61.261031
2085.798364	13257.350605	61.266036
2085.202915	13200.364067	61.271041
2084.916343	13130.103066	61.276046
2084.403891	13060.268868	61.281050
2083.285409	13012.956638	61.286055
2083.115326	12955.202052	61.291060
2082.204219	12889.357862	61.296065
2081.555598	12835.614687	61.301070
2080.971153	12773.212839	61.306074
2080.403574	12720.188753	61.311079
2079.937122	12648.047994	61.316084
2079.373444	12590.368591	61.321089
2078.774710	12517.197914	61.326094
2078.188542	12444.327439	61.331098
2077.062400	12387.494443	61.336103
2076.745482	12316.466097	61.341108
2075.859895	12258.801155	61.346113
2075.165449	12205.308163	61.351118
2074.657477	12136.231101	61.356122
2073.885998	12074.098536	61.361127
2073.190650	12005.147681	61.366132
2072.439234	11958.783745	61.371137
2071.981603	11904.510106	61.376142
2071.489470	11825.800143	61.381146
2070.487009	11770.637719	61.386151
2070.101129	11714.936153	61.391156
2069.952707	11662.437514	61.396161
2068.963663	11596.321209	61.401166
2068.672311	11530.247164	61.406170
2067.721575	11464.105038	61.411175
2067.138681	11391.340888	61.416180
2066.230841	11333.191406	61.421185
2065.601589	11270.807182	61.426190
2065.224616	11207.246134	61.431194
2064.428916	11153.833680	61.436199
2063.889407	11084.585322	61.441204
2063.627344	11022.797588	61.446209
2062.678115	10955.677042	61.451214
2062.163862	10888.086930	61.456218
2061.583203	10824.450135	61.461223
2060.665968	10759.391112	61.466228
2060.039911	10693.455696	61.471233
2059.412975	10627.607502	61.476238
2058.683712	10550.917939	61.481242
2057.945848	10499.739871	61.486247
2057.015509	10433.372176	61.491252
2056.635053	10371.386739	61.496257
2055.990735	10306.957029	61.501262
2055.284841	10241.661161	61.506266
2054.275905	10179.039506	61.511271
2054.087398	10126.817267	61.516276
2053.628445	10060.306581	61.521281
2052.591281	9984.348887	61.526286
2051.834902	9919.494013	61.531290
2050.876009	9865.900568	61.536295
2050.438867	9805.646271	61.541300
2049.841146	9744.870138	61.546305
2049.195302	9682.180702	61.551310
2048.824405	9616.974820	61.556314
2047.780113	9576.196060	61.561319
2047.473423	9510.368201	61.566324
2046.730987	9454.989549	61.571329
2046.163672	9381.844439	61.576334
2045.533426	9317.375705	61.581338
2044.690727	9266.140758	61.586343
2044.242046	9192.848350	61.591348
2043.520592	9130.028048	61.596353
2042.885240	9067.079550	61.601358
2042.098666	9006.907972	61.606362
2041.012090	8946.720341	61.611367
2040.804715	8888.200504	61.616372
2040.038510	8835.223943	61.621377
2039.462127	8772.745817	61.626382
2038.574244	8705.853582	61.631386
2037.679121	8657.423058	61.636391
2037.529298	8597.761916	61.641396
2036.916702	8544.027118	61.646401
2036.378342	8483.196577	61.651406
2035.610357	8413.002721	61.656410
2034.922802	8356.257347	61.661415
2034.134621	8294.230591	61.666420
2033.478183	8237.737915	61.671425
2032.738066	8180.215399	61.676430
2032.512371	8113.312630	61.681434
2031.565492	8054.202607	61.686439
2030.683562	7990.218946	61.691444
2030.000605	7938.395189	61.696449
2029.404791	7874.875847	61.701454
2028.892640	7822.392693	61.706458
2028.156708	7767.921741	61.711463
2027.721534	7694.832135	61.716468
2027.014851	7646.557611	61.721473
2026.195907	7586.324311	61.726478
2025.664248	7530.997429	61.731482
2025.099902	7475.944155	61.736487
2024.372338	7402.592357	61.741492
2023.700901	7342.092084	61.746497
2023.135589	7274.799682	61.751502
2022.535484	7220.325741	61.756506
2021.620545	7163.432848	61.761511
2021.058951	7096.755573	61.766516
2020.398888	7042.116675	61.771521
2019.544883	6978.334478	61.776526
2019.104597	6926.752610	61.781530
2018.241028	6861.888561	61.786535
2017.802711	6796.733274	61.791540
2017.101306	6741.791239	61.796545
2016.290110	6686.746931	61.801550
2016.258166	6631.194203	61.806554
2015.089650	6572.044388	61.811559
2014.797249	6509.009650	61.816564
2014.103517	6444.338183	61.821569
2013.361770	6382.597964	61.826574
2012.825299	6318.433747	61.831578
2011.676551	6254.941235	61.836583
2011.346142	6188.410794	61.841588
2010.911607	6138.134643	61.846593
2010.020989	6078.179924	61.851598
2009.237689	6008.989770	61.856602
2008.230990	5953.497259	61.861607
2007.999602	5885.319662	61.866612
2007.313733	5826.868445	61.871617
2006.558085	5767.549042	61.876622
2005.796338	5720.592586	61.881626
2005.363554	5664.575452	61.886631
2004.578442	5594.433893	61.891636
2003.797811	5539.951388	61.896641
2003.142593	5476.860302	61.901646
2002.809993	5409.947205	61.906650
2001.975258	5361.405442	61.911655
2001.787978	5288.131357	61.916660
2001.057205	5234.183941	61.921665
1999.992402	5165.838261	61.926670
1999.163555	5103.416791	61.931674
1998.120018	5051.494705	61.936679
1997.784927	4989.622400	61.941684
1996.743738	4936.029797	61.946689
1996.162707	4889.622290	61.951694
1996.012777	4822.107872	61.956698
1995.357423	4781.725002	61.961703
1994.955595	4715.013755	61.966708
1994.442374	4646.286375	61.971713
1993.517408	4595.536471	61.976718
1992.831129	4530.344534	61.981722
1992.136514	4474.048520	61.986727
1991.920654	4401.095697	61.991732
1990.791600	4350.428719	61.996737
1990.136703	4278.849917	62.001742
1989.617412	4218.727084	62.006746
1988.792937	4158.507815	62.011751
1988.068711	4107.842092	62.016756
1987.289006	4048.368582	62.021761
1986.186624	3984.775954	62.026766
1985.798331	3934.377716	62.031770
1985.221521	3885.389765	62.036775
1985.081320	3823.103388	62.041780
1983.978550	3775.709603	62.046785
1983.208180	3723.320599	62.051790
1982.676644	3651.254433	62.056794
1981.693871	3603.450191	62.061799
1981.026173	3552.584977	62.066804
1980.720213	3490.900463	62.071809
1980.046584	3440.304725	62.076814
1979.581420	3391.724209	62.081818
1978.909870	3323.028928	62.086823
1978.361791	3260.472919	62.091828
1977.377196	3211.116611	62.096833
1976.852849	3150.632230	62.101838
1976.184663	3083.093688	62.106842
1975.364744	3042.278791	62.111847
1974.805699	2971.430884	62.116852
1973.940141	2936.209411	62.121857
1973.447677	2872.935673	62.126862
1972.576946	2819.387623	62.131866
1971.816842	2762.767092	62.136871
1971.095738	2714.993618	62.141876
1970.619742	2664.179923	62.146881
1969.919653	2603.271454	62.151886
1969.507322	2544.500434	62.156890
1968.583211	2504.564740	62.161895
1968.073842	2442.006871	62.166900
1967.491400	2394.195087	62.171905
1966.503386	2325.214043	62.176910
1966.206562	2283.398732	62.181914
1965.296152	2226.477659	62.186919
1964.856692	2164.584915	62.191924
1964.051218	2116.948233	62.196929
1963.290953	2066.880423	62.201934
1963.029721	2021.625930	62.206938
1962.112217	1964.893109	62.211943
1961.361040	1904.811053	62.216948
1960.498921	1857.655777	62.221953
1960.067212	1806.481600	62.226958
1959.637559	1747.207909	62.231962
1958.573150	1701.216055	62.236967
1958.351064	1649.634586	62.241972
1957.465237	1593.563729	62.246977
1956.639534	1550.472628	62.251982
1956.378245	1481.024585	62.256986
1955.286280	1433.201415	62.261991
1954.523732	1390.408299	62.266996
1953.768096	1338.396126	62.272001
1953.118816	1288.508936	62.277006
1952.871989	1235.794993	62.282010
1951.822857	1191.040335	62.287015
1951.168063	1143.291452	62.292020
1950.633446	1099.157201	62.297025
1949.727406	1050.111157	62.302030
1949.424445	998.337449	62.307034
1948.234010	960.218514	62.312039
1947.773736	908.145226	62.317044
1947.013359	867.737794	62.322049
1946.295193	824.445689	62.327054
1945.831037	768.295312	62.332058
1944.838536	736.272299	62.337063
1944.957192	682.521436	62.342068
1943.775821	646.306928	62.347073
1943.017233	593.876829	62.352078
1942.502997	556.298193	62.357082
1941.715791	521.069349	62.362087
1940.862474	470.744259	62.367092
1940.017497	430.845075	62.372097
1939.514652	399.702314	62.377102
1939.184267	346.525455	62.382106
1938.029052	314.995993	62.387111
1937.769260	276.989756	62.392116
1937.013083	234.665825	62.397121
1936.269924	205.025058	62.402126
1935.519847	164.687341	62.407130
1935.147706	136.162655	62.412135
1934.267577	97.241380	62.417140
1933.274529	66.800049	62.422145
1932.335315	35.799883	62.427150
1931.572587	7.810539	62.432154
1930.329024	-2.530554	62.437159
1928.581754	-7.280265	62.442164
1927.081111	13.690247	62.447169
1926.327645	20.929977	62.452174
1925.929285	16.595328	62.457178
1925.622264	27.132545	62.462183
1925.224187	14.894199	62.467188
1925.139500	23.128472	62.472193
1924.313732	29.034549	62.477198
1923.527925	26.112846	62.482202
1922.515383	32.176308	62.487207
1921.617344	34.843775	62.492212
1921.645140	25.910904	62.497217
1920.791028	42.398068	62.502222
1920.518559	29.881151	62.507226
1919.449128	36.199650	62.512231
1918.432884	42.932331	62.517236
1918.206847	34.831378	62.522241
1917.683383	38.167933	62.527246
1917.401017	26.950418	62.532250
1916.280805	36.110752	62.537255
1915.398036	43.110826	62.542260
1914.904254	38.870167	62.547265
1913.939150	51.645483	62.552270
1914.189586	38.047341	62.557274
1913.454928	47.419287	62.562279
1912.915659	34.859567	62.567284
1912.180228	49.150136	62.572289
1911.012376	48.944665	62.577294
1910.586118	37.108169	62.582298
1909.870808	48.963891	62.587303
1909.022442	35.669498	62.592308
1908.504021	45.122234	62.597313
1907.706384	32.846384	62.602318
1907.391950	39.100223	62.607322
1906.253627	32.213273	62.612327
1905.584375	49.070068	62.617332
1905.267948	39.661982	62.622337
1905.475138	37.994008	62.627342
1904.009855	46.866937	62.632346
1903.024498	32.507781	62.637351
1902.743445	38.034079	62.642356
1902.671312	31.003100	62.647361
1901.150019	40.690737	62.652366
1900.499713	35.727459	62.657370
1900.040282	40.564567	62.662375
1900.053382	48.288167	62.667380
1898.929656	39.929184	62.672385
1897.724733	49.339522	62.677390
1897.623590	32.698499	62.682394
1897.270822	41.629773	62.687399
1896.044034	43.701315	62.692404
1895.270185	44.076694	62.697409
1895.094823	38.982822	62.702414
1894.309575	34.212857	62.707418
1892.988385	47.929373	62.712423
1893.085372	35.684962	62.717428
1892.642472	37.934830	62.722433
1891.429710	34.387062	62.727438
1890.811184	34.909671	62.732442
1890.544808	41.903355	62.737447
1889.380159	42.097929	62.742452
1888.718518	36.329057	62.747457
1888.576889	41.800107	62.752462
1887.883941	41.740022	62.757466
1886.436290	41.612099	62.762471
1886.516053	36.772614	62.767476
1886.033385	41.383178	62.772481
1884.952048	45.577859	62.777486
1884.390973	41.932938	62.782490
1883.445713	51.735719	62.787495
1882.834395	41.388862	62.792500
1882.613237	44.667967	62.797505
1881.560565	48.446515	62.802510
1881.182577	35.235152	62.807514
1880.398772	52.685725	62.812519
1879.691685	46.081976	62.817524
1879.144109	38.210273	62.822529
1878.561313	40.107040	62.827534
1878.102908	34.775835	62.832538
1877.577784	38.360241	62.837543
1877.099650	42.996895	62.842548
1876.075014	34.253189	62.847553
1874.699577	41.356723	62.852558
1874.480949	39.575004	62.857562
1873.850933	37.688289	62.862567
1872.978396	37.057481	62.867572
1872.617117	32.194981	62.872577
1871.423644	33.313499	62.877582
1871.314987	35.562342	62.882586
1870.455462	39.527845	62.887591
1869.833905	32.946797	62.892596
1869.594476	34.047885	62.897601
1868.591624	39.087967	62.902606
1868.460077	33.050439	62.907610
1868.066045	33.614680	62.912615
1867.128033	38.827394	62.917620
1866.003810	40.959935	62.922625
1864.846773	39.268861	62.927630
1864.823163	44.689634	62.932634
1863.769691	41.783637	62.937639
1863.217139	35.940683	62.942644
1863.256905	30.654968	62.947649
1862.394086	45.913509	62.952654
1861.804884	39.560712	62.957658
1860.944361	37.653828	62.962663
1859.582200	36.695488	62.967668
1859.214257	37.001700	62.972673
1858.478651	45.746182	62.977678
1858.472924	30.924009	62.982682
1857.418077	37.022595	62.987687
1856.896649	38.859161	62.992692
1856.018570	31.214984	62.997697
1855.514264	38.875646	63.002702
1855.204894	35.140308	63.007706
1854.432309	44.523016	63.012711
1853.502525	32.424290	63.017716
1852.384604	37.003255	63.022721
1852.013202	46.314382	63.027726
1851.676376	28.146463	63.032730
1850.500131	41.412622	63.037735
1850.007750	32.902965	63.042740
1849.249709	38.350459	63.047745
1848.455946	33.791596	63.052750
1848.143405	36.129581	63.057754
1847.658255	37.846848	63.062759
1847.135799	45.031004	63.067764
1846.924067	36.602941	63.072769
1846.221873	41.521178	63.077774
1845.433058	37.586000	63.082778
1844.207986	41.472357	63.087783
1843.180109	36.133809	63.092788
1843.088287	32.832285	63.097793
1842.347522	36.444626	63.102798
1841.699538	32.733093	63.107802
1841.190665	41.162456	63.112807
1840.467612	42.859151	63.117812
1839.357330	37.265608	63.122817
1838.389156	50.482972	63.127822
1838.397831	41.239322	63.132826
1837.692433	51.074992	63.137831
1837.091747	43.601237	63.142836
1836.516278	42.130069	63.147841
1835.839622	43.299007	63.152846
1835.787710	35.570965	63.157850
1834.689583	39.635865	63.162855
1833.738760	40.309019	63.167860
1832.863060	36.129023	63.172865
1831.909793	40.524158	63.177870
1831.904133	30.585782	63.182874
1831.103799	36.131458	63.187879
1830.472968	41.375833	63.192884
1830.236247	30.379746	63.197889
1829.523102	35.203529	63.202894
1828.656081	27.251682	63.207898
1827.783622	42.489679	63.212903
1827.123561	34.765163	63.217908
1826.546157	38.156029	63.222913
1825.880759	36.658143	63.227918
1825.553888	31.522108	63.232922
1824.094370	33.528133	63.237927
1823.214357	32.860683	63.242932
1823.088107	32.559246	63.247937
1822.282428	33.827521	63.252942
1821.740886	35.206818	63.257946
1821.463108	32.899913	63.262951
1821.146666	37.503013	63.267956
1820.669613	40.788060	63.272961
1819.585526	41.187492	63.277966
1818.532158	38.634734	63.282970
1817.818002	37.609792	63.287975
1817.136791	40.834217	63.292980
1816.866364	34.252623	63.297985
1815.977610	38.803098	63.302990
1815.348177	40.786131	63.307994
1814.050975	43.542246	63.312999
1813.540117	37.697415	63.318004
1813.194175	32.864030	63.323009
1812.065191	42.235528	63.328014
1812.114468	40.573701	63.333018
1811.581120	38.935002	63.338023
1810.991079	33.553754	63.343028
1810.817959	33.318107	63.348033
1809.594808	41.594389	63.353038
1808.811139	30.172649	63.358042
1807.738418	39.011667	63.363047
1807.176093	40.838966	63.368052
1806.962122	42.122097	63.373057
1806.251153	45.070555	63.378062
1805.575820	36.984196	63.383066
1804.332073	36.696207	63.388071
1803.492437	39.154165	63.393076
1803.330631	34.860819	63.398081
1802.863373	45.805115	63.403086
1802.353040	27.399838	63.408090
1801.609812	30.086913	63.413095
1801.381322	29.726018	63.418100
1800.310654	34.294345	63.423105
1799.346923	44.294040	63.428110
1798.916334	39.537174	63.433114
1798.414848	37.628493	63.438119
1797.737759	27.902397	63.443124
1796.568742	35.247572	63.448129
1795.439646	35.029691	63.453134
1795.189585	27.531818	63.458138
1794.518767	43.806970	63.463143
1794.126373	38.468456	63.468148
1793.779278	37.320577	63.473153
1793.133750	43.920313	63.478158
1793.263289	37.038666	63.483162
1791.937668	33.365369	63.488167
1791.013894	41.419077	63.493172
1790.747546	32.466691	63.498177
1789.560041	39.280223	63.503182
1788.571595	37.043597	63.508186
1787.830058	36.030895	63.513191
1787.250719	36.993580	63.518196
1787.082880	33.156932	63.523201
1786.284457	43.035761	63.528206
1786.279992	31.916068	63.533210
1785.607825	38.472724	63.538215
1784.882632	36.995383	63.543220
1784.114261	30.612718	63.548225
1783.020133	40.426541	63.553230
1782.002887	37.705638	63.558234
1780.925286	42.418577	63.563239
1780.543135	39.044890	63.568244
1780.434269	31.756407	63.573249
1779.743485	44.157026	63.578254
1779.359648	30.271693	63.583258
1778.880234	29.878109	63.588263
1777.849442	34.034837	63.593268
1777.005241	31.821041	63.598273
1775.883239	34.784315	63.603278
1775.810392	34.542209	63.608282
1775.022304	30.725212	63.613287
1774.764607	36.719313	63.618292
1774.590939	31.779731	63.623297
1773.054962	37.159971	63.628302
1772.314818	27.937482	63.633306
1771.612427	33.712044	63.638311
1771.052179	30.743532	63.643316
1771.028204	33.628630	63.648321
1769.898347	42.341118	63.653326
1769.172750	33.507399	63.658330
1768.494793	35.267913	63.663335
1767.857730	37.307360	63.668340
1767.416021	31.497294	63.673345
1766.331744	35.293516	63.678350
1765.378839	30.482414	63.683354
1764.783913	37.154540	63.688359
1764.322305	35.994889	63.693364
1763.995663	29.485311	63.698369
1763.464210	32.719080	63.703374
1763.078977	34.707497	63.708378
1761.983261	37.838489	63.713383
1760.976633	41.038913	63.718388
1760.761852	35.566545	63.723393
1759.968469	33.675843	63.728398
1759.724549	30.038937	63.733402
1758.442942	29.851599	63.738407
1757.815964	41.570308	63.743412
1757.358498	39.148445	63.748417
1756.363041	40.409031	63.753422
1756.402658	34.065213	63.758426
1755.175573	32.210274	63.763431
1754.277573	38.911610	63.768436
1754.088787	20.202985	63.773441
1753.115720	38.599814	63.778446
1753.002971	32.250233	63.783450
1752.526495	38.742702	63.788455
1751.512583	38.769896	63.793460
1750.604882	25.980171	63.798465
1749.922616	34.405537	63.803470
1749.625733	32.014944	63.808474
1748.886180	29.552728	63.813479
1747.175824	26.401026	63.818484
1747.013374	33.762979	63.823489
1746.158905	29.341527	63.828494
1745.726450	32.017108	63.833498
1745.441373	27.931004	63.838503
1745.076082	42.713157	63.843508
1744.930466	32.038506	63.848513
1743.936098	37.381632	63.853518
1742.820619	33.346983	63.858522
1742.029742	27.191835	63.863527
1741.535200	36.845790	63.868532
1740.866371	25.599809	63.873537
1740.153952	33.738230	63.878542
1739.641126	22.573130	63.883546
1738.894333	34.269863	63.888551
1738.286662	23.088288	63.893556
1737.249495	34.861100	63.898561
1735.896218	32.203047	63.903566
1736.022951	10.829757	63.908570
1735.064570	30.183027	63.913575
1734.664255	35.852852	63.918580
1734.574861	24.628388	63.923585
1734.114012	32.424082	63.928590
1733.662421	29.305861	63.933594
1732.393732	34.170588	63.938599
1731.737477	26.959588	63.943604
1731.189016	37.479965	63.948609
1729.738674	41.990349	63.953614
1729.379890	25.820795	63.958618
1728.797536	29.225078	63.963623
1728.349492	29.469914	63.968628
1728.074324	30.332263	63.973633
1727.126984	27.437858	63.978638
1726.401206	17.348947	63.983642
1725.962137	35.735083	63.988647
1725.361736	34.154363	63.993652
1724.263183	28.961136	63.998657
1723.054969	45.597611	64.003662
1722.612202	29.163853	64.008666
1722.149475	41.108789	64.013671
1721.572763	31.034042	64.018676
1721.449845	33.288306	64.023681
1720.448869	30.230534	64.028686
1719.941913	32.055363	64.033690
1718.679205	36.132253	64.038695
1718.320292	38.863967	64.043700
1718.150770	33.349724	64.048705
1716.703663	37.515826	64.053710
1715.859738	33.573677	64.058714
1715.513853	31.509415	64.063719
1714.824978	40.248074	64.068724
1714.733172	34.565371	64.073729
1714.166303	38.861326	64.078734
1713.400943	22.283274	64.083738
1712.700372	25.742605	64.088743
1711.548353	38.255908	64.093748
1711.371066	22.123769	64.098753
1710.116713	27.342616	64.103758
1709.453311	25.521173	64.108762
1708.981808	31.542925	64.113767
1708.130067	37.647149	64.118772
1708.102159	31.575832	64.123777
1707.372154	40.481874	64.128782
1706.825446	32.316776	64.133786
1705.793269	38.121655	64.138791
1705.102705	39.538837	64.143796
1704.888976	27.627653	64.148801
1703.654385	34.093881	64.153806
1702.850425	26.322882	64.158810
1702.409795	34.120100	64.163815
1701.835530	27.925831	64.168820
1701.538866	31.579631	64.173825
1700.838277	32.044355	64.178830
1699.842821	27.687892	64.183834
1698.995359	36.722975	64.188839
1698.579829	33.876574	64.193844
1698.378219	29.121211	64.198849
1697.333519	29.113894	64.203854
1696.545189	26.329861	64.208858
1695.727256	32.950685	64.213863
1695.475321	28.566013	64.218868
1695.111611	21.239176	64.223873
1693.866587	41.776548	64.228878
1693.046509	23.680714	64.233882
1692.145377	38.212082	64.238887
1691.765401	30.665476	64.243892
1691.651394	15.726506	64.248897
1690.538176	33.775020	64.253902
1689.621606	31.290477	64.258906
1689.242649	21.588034	64.263911
1688.395114	33.939437	64.268916
1688.122858	28.643367	64.273921
1687.635715	31.725032	64.278926
1687.010674	29.783961	64.283930
1686.013274	27.275989	64.288935
1685.334214	31.313803	64.293940
1685.117713	14.319013	64.298945
1683.904160	31.465683	64.303950
1683.112017	24.621635	64.308954
1682.491439	29.011279	64.313959
1682.121814	19.502898	64.318964
1682.048115	25.603388	64.323969
1680.694799	36.246881	64.328974
1679.731220	21.122734	64.333978
1679.284314	29.830844	64.338983
1678.926171	29.682942	64.343988
1678.946566	34.398127	64.348993
1677.372789	23.994499	64.353998
1676.630485	21.299357	64.359002
1676.031471	29.131194	64.364007
1675.754452	32.953763	64.369012
1674.571870	26.928667	64.374017
1673.347097	40.065393	64.379022
1673.010400	24.237702	64.384026
1672.233871	32.389472	64.389031
1672.121887	29.337167	64.394036
1671.657979	33.367616	64.399041
1671.469577	44.729668	64.404046
1670.462142	31.474852	64.409050
1669.601188	35.098442	64.414055
1669.123972	31.941726	64.419060
1668.619585	30.776274	64.424065
1667.401618	41.141235	64.429070
1666.750949	30.283475	64.434074
1665.837633	36.785419	64.439079
1665.453048	35.709746	64.444084
1665.280167	30.408932	64.449089
1664.101528	34.089294	64.454094
1663.337423	27.220298	64.459098
1662.873976	27.488092	64.464103
1662.418765	30.201991	64.469108
1662.250968	28.398029	64.474113
1660.650174	36.825815	64.479118
1660.041126	28.869330	64.484122
1659.579139	31.915464	64.489127
1658.835784	39.040113	64.494132
1658.709081	32.811029	64.499137
1657.589140	37.805125	64.504142
1656.757767	27.200002	64.509146
1656.184827	31.096386	64.514151
1655.501789	36.404278	64.519156
1655.167907	26.328830	64.524161
1654.476784	28.969819	64.529166
1653.375304	29.673277	64.534170
1652.884153	25.329766	64.539175
1652.188973	34.755404	64.544180
1652.325741	17.354421	64.549185
1650.540687	28.426045	64.554190
1650.003205	17.190779	64.559194
1649.718765	36.064855	64.564199
1648.965520	22.810680	64.569204
1648.966412	24.734620	64.574209
1647.999024	28.152773	64.579214
1647.363154	34.804612	64.584218
1646.606140	32.875053	64.589223
1645.939291	29.269077	64.594228
1644.996673	18.194362	64.599233
1644.137230	25.361102	64.604238
1643.899325	17.891293	64.609242
1643.353831	22.565480	64.614247
1642.611194	26.867288	64.619252
1641.885174	21.540810	64.624257
1640.836577	34.912904	64.629262
1640.095272	24.780758	64.634266
1639.956399	15.877548	64.639271
1638.806690	32.626163	64.644276
1638.369007	25.066662	64.649281
1637.466170	30.272278	64.654286
1637.352152	22.262397	64.659290
1636.913865	26.817054	64.664295
1636.280123	25.967046	64.669300
1635.278548	28.466547	64.674305
1634.421516	25.852720	64.679310
1634.282494	32.726828	64.684314
1633.267983	23.139554	64.689319
1632.226036	26.531709	64.694324
1631.626641	27.142801	64.699329
1630.792019	24.181643	64.704334
1630.641612	27.793290	64.709338
1630.320611	24.405189	64.714343
1629.139377	29.973575	64.719348
1628.438540	29.496923	64.724353
1627.971451	37.943322	64.729358
1627.924675	26.917106	64.734362
1626.636252	33.901269	64.739367
1625.637036	27.955878	64.744372
1625.171027	24.210771	64.749377
1624.329915	36.114893	64.754382
1624.290578	28.118378	64.759386
1623.679402	29.844663	64.764391
1622.676307	34.161047	64.769396
1622.293526	22.450205	64.774401
1621.374273	30.924277	64.779406
1620.578790	27.813403	64.784410
1619.861755	27.075978	64.789415
1619.151326	30.633091	64.794420
1619.024785	34.783417	64.799425
1618.349489	29.876236	64.804430
1617.295538	36.704885	64.809434
1617.086367	28.044650	64.814439
1615.949562	36.091244	64.819444
1615.433082	32.401463	64.824449
1614.196052	31.937459	64.829454
1613.521572	30.180879	64.834458
1613.421943	30.241074	64.839463
1612.759799	31.555993	64.844468
1612.639836	30.722139	64.849473
1611.297420	39.533101	64.854478
1610.913950	22.697311	64.859482
1610.269787	31.599189	64.864487
1609.563480	32.714545	64.869492
1608.583546	26.334018	64.874497
1607.740009	38.952885	64.879502
1607.405491	28.152155	64.884506
1607.072723	30.241065	64.889511
1606.481232	32.093537	64.894516
1605.586126	27.137704	64.899521
1604.775634	33.227515	64.904526
1604.259023	33.528997	64.909530
1603.741225	38.119948	64.914535
1602.557269	34.474710	64.919540
1601.945911	28.538673	64.924545
1601.164228	36.388507	64.929550
1601.062897	30.959641	64.934554
1600.538402	27.066136	64.939559
1599.546832	27.845195	64.944564
1598.925191	30.050961	64.949569
1598.141789	46.746138	64.954574
1597.901124	20.582131	64.959578
1596.733695	29.887261	64.964583
1595.707447	30.416367	64.969588
1595.550192	24.570614	64.974593
1594.908487	34.826697	64.979598
1594.699652	28.817251	64.984602
1593.962876	30.842616	64.989607
1592.997682	31.508678	64.994612
1592.544734	27.408268	64.999617
1591.381619	23.408070	65.004622
1590.385988	24.222470	65.009626
1589.376000	26.912557	65.014631
1589.339157	20.126743	65.019636
1588.954546	25.002459	65.024641
1588.413279	27.944504	65.029646
1588.383807	26.773002	65.034650
1587.622167	21.770743	65.039655
1586.446858	36.929157	65.044660
1585.916530	20.203442	65.049665
1584.737106	30.431415	65.054670
1584.137017	13.756215	65.059674
1583.343451	24.842236	65.064679
1582.978583	29.662778	65.069684
1582.965131	21.622734	65.074689
1581.927481	32.742809	65.079694
1581.205076	32.362637	65.084698
1580.550924	29.259284	65.089703
1579.997185	33.743984	65.094708
1578.841941	19.840935	65.099713
1577.998903	20.785636	65.104718
1577.731043	24.073748	65.109722
1577.599855	21.647394	65.114727
1576.412327	31.208035	65.119732
1575.797669	20.503867	65.124737
1575.000192	27.643434	65.129742
1574.777420	26.015369	65.134746
1574.024703	20.656886	65.139751
1572.716061	35.407560	65.144756
1572.315430	24.850732	65.149761
1571.446162	31.416664	65.154766
1571.331661	34.167907	65.159770
1570.776371	21.793788	65.164775
1569.852699	31.878632	65.169780
1569.429919	21.334788	65.174785
1568.604554	21.688486	65.179790
1568.035291	21.801222	65.184794
1566.834923	30.431936	65.189799
1566.193895	24.324008	65.194804
1565.737991	29.805561	65.199809
1565.358966	28.801561	65.204814
1565.240515	26.358990	65.209818
1564.153834	21.238074	65.214823
1563.141801	26.068401	65.219828
1562.562922	19.655715	65.224833
1561.099646	32.721556	65.229838
1560.695486	26.320530	65.234842
1560.399936	23.764175	65.239847
1559.598432	22.844648	65.244852
1559.497031	17.570342	65.249857
1559.114475	30.019774	65.254862
1558.500604	21.966322	65.259866
1557.729404	26.725271	65.264871
1556.713692	32.229540	65.269876
1556.034052	15.098638	65.274881
1554.904501	25.951047	65.279886
1554.822567	16.040601	65.284890
1554.014424	19.636906	65.289895
1553.302261	28.190053	65.294900
1552.384177	19.418548	65.299905
1551.607317	19.755082	65.304910
1551.381631	23.842311	65.309914
1551.069082	28.432194	65.314919
1550.127384	22.528162	65.319924
1549.298138	18.993751	65.324929
1548.596978	21.475511	65.329934
1548.235691	24.113002	65.334938
1548.240682	31.009956	65.339943
1546.670745	28.201931	65.344948
1545.937876	22.203220	65.349953
1545.215333	31.013483	65.354958
1544.774697	23.405591	65.359962
1543.774043	19.906302	65.364967
1542.710590	18.367665	65.369972
1542.763131	19.703082	65.374977
1542.184715	19.552353	65.379982
1541.840414	26.302956	65.384986
1541.031715	23.397635	65.389991
1539.994880	31.887258	65.394996
1539.742313	24.541217	65.400001
1538.917435	34.362793	65.405006
1537.782600	24.848300	65.410010
1537.192507	27.511110	65.415015
1536.877987	27.677992	65.420020
1536.540278	33.158115	65.425025
1535.418935	32.431341	65.430030
1534.635078	25.494570	65.435034
1533.793100	22.129343	65.440039
1533.462795	21.994384	65.445044
1533.306022	22.983018	65.450049
1531.898300	32.484047	65.455054
1531.338072	22.860909	65.460058
1530.860720	23.112013	65.465063
1529.972874	25.287554	65.470068
1530.180375	17.352756	65.475073
1529.187754	28.555574	65.480078
1528.727365	29.210832	65.485082
1528.026398	29.070117	65.490087
1526.753952	30.007374	65.495092
1526.300508	18.288867	65.500097
1525.490933	33.001253	65.505102
1525.003340	33.889492	65.510106
1523.826388	21.885405	65.515111
1523.326788	36.625810	65.520116
1522.829898	21.170550	65.525121
1522.404879	36.603995	65.530126
1521.757802	25.682645	65.535130
1520.753811	23.141097	65.540135
1519.809120	27.053999	65.545140
1519.772808	18.874094	65.550145
1519.042678	26.337283	65.555150
1518.817443	27.956533	65.560154
1517.911308	31.245150	65.565159
1517.031858	25.171969	65.570164
1516.588164	29.789002	65.575169
1515.227885	29.781442	65.580174
1514.700118	22.638408	65.585178
1514.108033	20.390952	65.590183
1513.337339	26.614807	65.595188
1513.435669	14.464855	65.600193
1513.016657	21.460717	65.605198
1511.849654	26.839231	65.610202
1511.361094	36.098019	65.615207
1510.360711	25.718513	65.620212
1510.019699	18.284034	65.625217
1508.795380	24.198353	65.630222
1508.383284	25.084059	65.635226
1508.093988	32.477202	65.640231
1506.923095	31.389311	65.645236
1506.237598	21.642586	65.650241
1505.727647	26.069877	65.655246
1505.250443	26.852390	65.660250
1504.822214	20.516704	65.665255
1503.435483	28.461124	65.670260
1503.101893	26.579444	65.675265
1502.231930	26.150203	65.680270
1501.870595	34.010530	65.685274
1501.544232	23.049264	65.690279
1500.672958	33.937922	65.695284
1499.880548	17.895705	65.700289
1499.346984	23.353334	65.705294
1498.363671	27.614576	65.710298
1497.508212	34.447991	65.715303
1496.588521	28.671369	65.720308
1496.481909	14.592274	65.725313
1495.926479	24.005184	65.730318
1495.685856	29.742692	65.735322
1494.608166	23.620599	65.740327
1493.604843	32.786149	65.745332
1493.443137	9.019220	65.750337
1493.055904	22.612669	65.755342
1491.828085	27.843161	65.760346
1491.286035	27.569971	65.765351
1490.520926	30.492413	65.770356
1489.869825	24.031299	65.775361
1488.843027	25.960855	65.780366
1488.471603	25.556472	65.785370
1487.981270	25.202525	65.790375
1487.477837	18.613870	65.795380
1487.141344	31.746683	65.800385
1486.087822	25.751640	65.805390
1485.615609	24.041800	65.810394
1484.678498	23.039770	65.815399
1483.558088	30.225947	65.820404
1483.494044	18.122299	65.825409
1482.857415	30.153220	65.830414
1482.402287	25.553291	65.835418
1481.460862	27.393590	65.840423
1480.612730	28.250823	65.845428
1480.250607	13.166828	65.850433
1479.226014	29.871943	65.855438
1478.329115	25.766417	65.860442
1477.769547	20.441928	65.865447
1477.365419	32.371247	65.870452
1477.369014	10.325300	65.875457
1476.051548	24.281045	65.880462
1475.172478	32.316689	65.885466
1475.011886	23.044795	65.890471
1473.967867	24.526089	65.895476
1473.728716	21.257469	65.900481
1472.631151	37.434878	65.905486
1471.936021	16.458744	65.910490
1471.516178	23.656589	65.915495
1470.691328	26.591684	65.920500
1469.951445	29.344544	65.925505
1469.392881	20.687826	65.930510
1468.960099	20.178082	65.935514
1468.428373	27.996101	65.940519
1467.328188	27.090954	65.945524
1466.629084	22.733228	65.950529
1465.753775	33.233032	65.955534
1465.648324	26.749863	65.960538
1465.151342	27.276908	65.965543
1464.089243	27.699800	65.970548
1463.919951	18.588564	65.975553
1463.063259	26.366765	65.980558
1462.092048	23.857879	65.985562
1461.613736	19.091332	65.990567
1460.695897	22.045937	65.995572
1460.423657	27.342196	66.000577
1459.572128	27.329506	66.005582
1458.249284	22.362865	66.010586
1457.917928	14.157320	66.015591
1457.410474	29.349972	66.020596
1457.168124	19.794612	66.025601
1456.630688	31.365075	66.030606
1455.565455	26.698112	66.035610
1455.050322	30.564845	66.040615
1454.469636	23.848127	66.045620
1453.555813	18.925295	66.050625
1452.549700	32.142451	66.055630
1452.222055	25.784483	66.060634
1451.792018	28.027638	66.065639
1451.107675	26.881370	66.070644
1450.547336	28.479766	66.075649
1449.527567	28.268315	66.080654
1449.016595	31.453151	66.085658
1448.711622	26.769442	66.090663
1447.568916	21.605447	66.095668
1446.631027	33.966525	66.100673
1445.941343	21.082382	66.105678
1445.756404	25.158408	66.110682
1445.315400	19.212695	66.115687
1443.774916	30.655572	66.120692
1443.702013	20.209121	66.125697
1443.013208	33.954588	66.130702
1442.688671	23.543397	66.135706
1442.259380	20.355463	66.140711
1440.842732	27.379003	66.145716
1440.427476	22.181397	66.150721
1440.121096	35.181694	66.155726
1439.165134	29.056049	66.160730
1438.667372	27.183124	66.165735
1438.059602	28.702330	66.170740
1437.297409	13.368122	66.175745
1436.148317	26.713656	66.180750
1435.802043	22.564789	66.185754
1435.271750	19.709874	66.190759
1433.961601	29.384669	66.195764
1433.696820	20.353268	66.200769
1432.910655	28.959199	66.205774
1432.179346	14.058472	66.210778
1432.432526	31.069867	66.215783
1431.191648	30.817872	66.220788
1430.587890	16.994420	66.225793
1430.230789	22.442936	66.230798
1429.136898	27.358858	66.235802
1428.088932	17.958355	66.240807
1427.198427	25.150587	66.245812
1427.139633	21.900616	66.250817
1426.768753	27.751866	66.255822
1426.227587	27.765552	66.260826
1425.759136	18.801217	66.265831
1424.642154	28.957819	66.270836
1424.367960	12.487931	66.275841
1422.705484	28.461818	66.280846
1422.246112	25.004281	66.285850
1421.827464	23.788984	66.290855
1421.198844	34.661170	66.295860
1421.039435	17.487066	66.300865
1419.787177	23.457901	66.305870
1419.156461	24.482445	66.310874
1418.854436	18.538303	66.315879
1417.912276	29.591206	66.320884
1417.378625	17.650517	66.325889
1416.571058	24.058448	66.330894
1415.724368	21.466711	66.335898
1415.702108	25.567345	66.340903
1414.275125	33.139740	66.345908
1414.120933	16.765893	66.350913
1413.569292	35.827493	66.355918
1412.583966	21.086990	66.360922
1412.098913	28.656326	66.365927
1410.804468	24.798516	66.370932
1410.587298	18.188036	66.375937
1409.923101	21.588039	66.380942
1409.635996	19.758909	66.385946
1408.681809	27.402811	66.390951
1407.833730	28.230097	66.395956
1407.517975	28.228459	66.400961
1407.033367	27.081995	66.405966
1406.104516	36.711971	66.410970
1405.342541	22.557283	66.415975
1404.613950	38.521524	66.420980
1404.473705	30.206758	66.425985
1403.225518	33.958206	66.430990
1402.495027	34.195953	66.435994
1401.904573	32.063381	66.440999
1401.241273	32.304640	66.446004
1401.367437	34.356896	66.451009
1400.069392	40.450140	66.456014
1399.240324	28.690444	66.461018
1399.261902	32.167529	66.466023
1398.025142	27.986745	66.471028
1397.363162	23.772949	66.476033
1396.642781	22.394307	66.481038
1396.154528	29.931039	66.486042
1395.845048	16.117596	66.491047
1395.116057	16.624762	66.496052
1394.388317	20.828067	66.501057
1393.840614	30.936771	66.506062
1392.344464	28.822007	66.511066
1391.843290	19.339340	66.516071
1391.299897	28.520118	66.521076
1390.957094	23.006657	66.526081
1390.764602	31.188654	66.531086
1389.347912	27.276169	66.536090
1389.241925	33.490592	66.541095
1388.262582	25.463748	66.546100
1387.651125	27.316284	66.551105
1386.802446	31.729628	66.556110
1386.047854	33.239067	66.561114
1385.945192	18.902322	66.566119
1384.847135	32.518882	66.571124
1383.948842	28.965542	66.576129
1383.189628	33.156510	66.581134
1382.968378	24.105582	66.586138
1382.647159	25.021016	66.591143
1381.700294	23.091759	66.596148
1381.065477	23.765307	66.601153
1380.227117	23.154468	66.606158
1379.877712	35.135018	66.611162
1379.212091	27.879893	66.616167
1377.758440	31.119968	66.621172
1377.324347	18.756617	66.626177
1376.960511	26.546382	66.631182
1376.655153	27.033523	66.636186
1375.843220	19.314387	66.641191
1374.951624	29.285370	66.646196
1374.963303	21.690778	66.651201
1373.510775	26.398804	66.656206
1372.591555	36.047757	66.661210
1372.193524	18.094741	66.666215
1371.590465	38.359835	66.671220
1371.287981	28.304694	66.676225
1370.836394	24.481658	66.681230
1369.667034	27.162466	66.686234
1369.416251	23.176625	66.691239
1368.653606	32.685571	66.696244
1367.637745	25.601242	66.701249
1366.739237	25.646512	66.706254
1366.458350	22.600581	66.711258
1366.121215	20.385175	66.716263
1364.853646	23.617753	66.721268
1364.219242	26.885300	66.726273
1363.591550	26.192093	66.731278
1363.239026	24.344983	66.736282
1362.735297	14.550500	66.741287
1361.657936	26.870685	66.746292
1361.153130	29.266086	66.751297
1360.654126	32.182532	66.756302
1359.951208	24.490225	66.761306
1358.728460	21.329091	66.766311
1357.895706	24.219743	66.771316
1357.888849	30.435752	66.776321
1357.159523	24.926970	66.781326
1356.874476	34.418345	66.786330
1356.134084	25.207098	66.791335
1355.101266	35.268347	66.796340
1354.716768	40.323843	66.801345
1354.251947	31.194941	66.806350
1353.150141	33.494438	66.811354
1352.660582	25.244673	66.816359
1352.072150	35.262089	66.821364
1351.354814	28.385774	66.826369
1350.578810	26.640677	66.831374
1349.929337	24.296731	66.836378
1349.985224	17.351121	66.841383
1348.650257	30.473923	66.846388
1348.181316	26.376110	66.851393
1347.137338	26.755169	66.856398
1346.063890	30.846290	66.861402
1345.573809	23.427657	66.866407
1344.980594	30.189458	66.871412
1344.367412	25.017028	66.876417
1344.139327	28.279911	66.881422
1343.494766	21.021454	66.886426
1342.857556	15.037572	66.891431
1341.997039	30.975476	66.896436
1341.661212	26.869118	66.901441
1341.047410	29.483698	66.906446
1340.036484	27.638756	66.911450
1339.267334	31.115385	66.916455
1338.696825	30.193900	66.921460
1338.289412	23.504864	66.926465
1337.141497	22.649940	66.931470
1336.269724	25.915804	66.936474
1336.146178	17.224668	66.941479
1335.450549	30.941267	66.946484
1334.861575	17.692659	66.951489
1333.912192	21.934369	66.956494
1333.283014	32.387188	66.961498
1333.052536	21.932687	66.966503
1331.811422	27.105437	66.971508
1331.381202	16.540770	66.976513
1331.037303	25.323990	66.981518
1330.391297	19.106546	66.986522
1329.706944	25.086484	66.991527
1328.233528	30.520091	66.996532
1327.954725	16.991945	67.001537
1327.495436	28.775495	67.006542
1326.844092	26.329351	67.011546
1326.109487	18.520673	67.016551
1325.321251	30.561521	67.021556
1325.154218	21.396332	67.026561
1324.524930	12.843948	67.031566
1323.320790	21.666155	67.036570
1322.944885	18.178025	67.041575
1322.043348	18.288447	67.046580
1321.868782	14.960696	67.051585
1320.793877	25.897530	67.056590
1320.059724	13.110401	67.061594
1319.610489	14.664351	67.066599
1318.841887	26.787230	67.071604
1318.286086	14.873754	67.076609
1317.403659	17.092654	67.081614
1316.655031	19.441670	67.086618
1316.563315	17.141524	67.091623
1315.494271	30.425487	67.096628
1315.000057	15.167001	67.101633
1314.570004	18.696955	67.106638
1313.351878	24.026904	67.111642
1312.342404	20.909158	67.116647
1311.632890	31.029402	67.121652
1311.401845	20.869884	67.126657
1311.161248	12.777675	67.131662
1310.547626	30.210687	67.136666
1310.531309	18.506329	67.141671
1309.446884	26.633006	67.146676
1308.771152	29.631172	67.151681
1307.445074	31.743994	67.156686
1306.464954	24.534166	67.161690
1306.749837	12.378231	67.166695
1305.887836	7.950266	67.171700
1305.225600	24.022223	67.176705
1304.296189	20.639441	67.181710
1303.902501	22.465258	67.186714
1303.283683	24.248021	67.191719
1301.885415	26.033281	67.196724
1301.588919	18.926080	67.201729
1300.999374	19.791144	67.206734
1300.875979	27.668841	67.211738
1299.928000	14.628713	67.216743
1298.925282	24.372952	67.221748
1298.709901	26.487386	67.226753
1297.842706	19.461458	67.231758
1296.701546	25.004679	67.236762
1296.143484	23.475682	67.241767
1295.572188	28.978766	67.246772
1295.496127	19.105268	67.251777
1294.575328	17.039439	67.256782
1293.266082	28.589122	67.261786
1293.098543	21.492957	67.266791
1292.065923	19.555293	67.271796
1292.234618	20.280883	67.276801
1291.324521	19.399208	67.281806
1290.297257	16.189685	67.286810
1289.993191	16.249280	67.291815
1289.212039	27.167805	67.296820
1288.367117	29.279830	67.301825
1287.744932	32.548606	67.306830
1286.778578	20.818680	67.311834
1286.639509	11.530787	67.316839
1285.993732	22.027244	67.321844
1285.176141	26.792059	67.326849
1284.681895	16.089354	67.331854
1284.250752	21.414037	67.336858
1283.322457	13.453248	67.341863
1282.525254	14.638334	67.346868
1281.746493	22.617073	67.351873
1281.429746	19.594203	67.356878
1280.247987	25.457695	67.361882
1279.827993	17.630552	67.366887
1279.249746	22.603315	67.371892
1279.110094	12.350432	67.376897
1277.913407	15.437739	67.381902
1276.810824	17.352616	67.386906
1276.677211	9.736985	67.391911
1276.074441	25.838914	67.396916
1275.352219	23.244784	67.401921
1274.863685	21.925509	67.406926
1274.161774	17.714947	67.411930
1273.853285	23.289786	67.416935
1272.788706	24.104231	67.421940
1271.645202	27.930554	67.426945
1271.459093	24.205677	67.431950
1270.238439	30.218861	67.436954
1269.663299	22.482617	67.441959
1268.511193	21.396582	67.446964
1268.380468	19.340758	67.451969
1268.081187	18.425050	67.456974
1267.841258	19.980422	67.461978
1267.390118	17.854121	67.466983
1266.160063	27.623480	67.471988
1265.682761	9.336191	67.476993
1265.140842	12.063932	67.481998
1263.890774	23.662560	67.487002
1263.800455	21.160347	67.492007
1262.673468	22.396298	67.497012
1261.867021	9.863540	67.502017
1261.017930	18.544160	67.507022
1260.421324	19.208508	67.512026
1260.156188	12.470066	67.517031
1259.422062	26.798333	67.522036
1258.851495	24.604290	67.527041
1258.239807	23.949566	67.532046
1257.451185	23.513784	67.537050
1257.047166	21.351607	67.542055
1256.035890	24.067250	67.547060
1255.469981	8.635691	67.552065
1254.905870	20.866408	67.557070
1254.047853	28.253792	67.562074
1253.673617	18.804599	67.567079
1252.392351	18.305228	67.572084
1252.595193	25.503430	67.577089
1251.853694	26.261780	67.582094
1250.530176	27.801796	67.587098
1250.144408	24.679519	67.592103
1249.194067	27.530553	67.597108
1249.016783	23.501504	67.602113
1248.685930	17.164591	67.607118
1247.418722	23.956304	67.612122
1247.175273	14.778052	67.617127
1246.316151	20.192867	67.622132
1245.446117	14.249192	67.627137
1244.531633	13.040230	67.632142
1244.043610	14.833746	67.637146
1244.185390	19.050211	67.642151
1243.161525	22.382864	67.647156
1242.408426	13.514308	67.652161
1241.816728	19.883223	67.657166
1240.503325	23.602534	67.662170
1239.763122	16.296245	67.667175
1239.027868	15.137632	67.672180
1238.376273	25.483638	67.677185
1238.277434	6.778221	67.682190
1237.761948	23.555389	67.687194
1237.649154	14.835751	67.692199
1236.524334	15.590404	67.697204
1235.791870	23.249559	67.702209
1235.512589	11.356798	67.707214
1234.091736	27.320738	67.712218
1233.680120	7.635317	67.717223
1232.746302	11.661696	67.722228
1232.423132	16.060900	67.727233
1231.653511	15.576374	67.732238
1230.783846	24.712857	67.737242
1230.235422	25.104626	67.742247
1229.914201	25.939654	67.747252
1229.531485	31.299223	67.752257
1228.577143	22.448474	67.757262
1227.959715	20.777549	67.762266
1227.330426	23.441922	67.767271
1226.229201	26.389496	67.772276
1225.453094	19.047920	67.777281
1225.251157	31.342480	67.782286
1224.686195	19.629183	67.787290
1223.869666	14.653129	67.792295
1222.812607	30.693267	67.797300
1222.153751	23.020812	67.802305
1221.801788	25.210584	67.807310
1221.183834	29.341283	67.812314
1220.304281	16.984163	67.817319
1219.694533	30.387501	67.822324
1219.552924	24.436808	67.827329
1218.969713	22.432441	67.832334
1217.722941	34.005338	67.837338
1217.126221	17.768140	67.842343
1216.577964	30.387426	67.847348
1216.117066	25.324858	67.852353
1215.075937	22.896575	67.857358
1214.272654	25.211733	67.862362
1213.979567	22.528882	67.867367
1212.768198	25.158089	67.872372
1211.839484	30.962449	67.877377
1211.382151	11.845690	67.882382
1211.015778	24.133277	67.887386
1210.713272	14.655344	67.892391
1210.475618	22.212165	67.897396
1209.991662	22.984765	67.902401
1208.627268	21.363243	67.907406
1208.082544	13.801957	67.912410
1207.609236	12.710507	67.917415
1206.448377	26.291367	67.922420
1205.978507	14.421035	67.927425
1205.460906	22.806109	67.932430
1204.621754	22.528188	67.937434
1204.131062	19.282258	67.942439
1203.187352	23.721802	67.947444
1202.483501	14.946352	67.952449
1201.628267	21.708840	67.957454
1200.622675	29.442978	67.962458
1200.633584	20.525476	67.967463
1200.190327	32.202408	67.972468
1200.076246	9.986011	67.977473
1198.823152	18.998972	67.982478
1197.960364	22.985684	67.987482
1197.907224	19.999753	67.992487
1196.521047	31.730441	67.997492
1195.509489	16.331921	68.002497
1195.245175	20.936233	68.007502
1194.608829	21.504415	68.012506
1194.386316	16.697255	68.017511
1193.053529	25.678741	68.022516
1192.601889	23.443725	68.027521
1192.064528	25.276636	68.032526
1192.032567	12.518241	68.037530
1190.981542	8.626576	68.042535
1189.931545	21.781382	68.047540
1189.453310	15.854267	68.052545
1189.136146	23.083116	68.057550
1188.057781	24.702446	68.062554
1187.872271	9.708728	68.067559
1186.802710	27.751985	68.072564
1185.794444	11.193907	68.077569
1185.193920	12.089127	68.082574
1184.764795	18.541005	68.087578
1184.387843	13.496637	68.092583
1183.627667	31.334580	68.097588
1182.515941	16.015076	68.102593
1181.974348	12.545439	68.107598
1181.439782	18.883201	68.112602
1181.280757	19.550516	68.117607
1180.371919	8.574742	68.122612
1179.436123	14.284039	68.127617
1178.938070	13.030952	68.132622
1178.097382	19.043665	68.137626
1177.994293	13.049009	68.142631
1176.995142	21.819747	68.147636
1176.507339	13.106143	68.152641
1175.472140	18.258824	68.157646
1174.843882	13.527234	68.162650
1174.434763	8.306638	68.167655
1173.736926	12.333352	68.172660
1172.769445	15.923564	68.177665
1172.053467	16.464992	68.182670
1171.423288	15.286536	68.187674
1171.304567	13.774429	68.192679
1169.954346	19.144368	68.197684
1169.097876	13.830916	68.202689
1168.886407	16.521891	68.207694
1168.187287	18.197607	68.212698
1168.075433	13.101620	68.217703
1166.949553	23.758027	68.222708
1166.187975	12.880261	68.227713
1165.853183	13.436760	68.232718
1164.903455	22.434605	68.237722
1164.207909	11.909033	68.242727
1163.468882	13.980599	68.247732
1163.183450	13.496359	68.252737
1162.731315	15.257373	68.257742
1161.641717	15.001951	68.262746
1161.043601	6.831017	68.267751
1160.104527	19.564493	68.272756
1160.195214	16.174073	68.277761
1159.280906	8.121234	68.282766
1158.008445	15.437358	68.287770
1157.934335	11.410837	68.292775
1157.173826	6.425902	68.297780
1156.466354	17.747459	68.302785
1155.606175	8.888086	68.307790
1155.114276	12.692820	68.312794
1154.540968	14.687570	68.317799
1153.635597	18.554912	68.322804
1152.829863	9.016684	68.327809
1152.414626	10.686677	68.332814
1152.172210	27.467729	68.337818
1151.344807	9.881132	68.342823
1150.125047	9.949188	68.347828
1149.478843	19.573688	68.352833
1149.508516	18.159405	68.357838
1148.570288	13.620622	68.362842
1147.655982	4.443439	68.367847
1147.055175	10.356505	68.372852
1146.529681	8.727749	68.377857
1146.266627	11.565698	68.382862
1145.105739	16.055569	68.387866
1144.785318	4.208803	68.392871
1143.990196	20.180479	68.397876
1142.790272	10.119909	68.402881
1142.225256	9.541368	68.407886
1141.384463	15.432683	68.412890
1141.286042	11.701762	68.417895
1140.643992	19.430132	68.422900
1140.203239	12.114101	68.427905
1138.992431	9.919419	68.432910
1138.541296	3.472356	68.437914
1138.536103	8.415494	68.442919
1137.454284	15.870037	68.447924
1136.736760	4.163702	68.452929
1136.206534	10.385660	68.457934
1135.106284	18.533832	68.462938
1134.585457	20.435085	68.467943
1133.848013	24.685728	68.472948
1133.462897	16.736383	68.477953
1132.596381	4.687898	68.482958
1131.562254	13.052629	68.487962
1131.474785	5.130065	68.492967
1130.851985	17.214008	68.497972
1130.001443	18.776625	68.502977
1129.150758	5.077731	68.507982
1128.442059	15.997369	68.512986
1127.959035	10.219266	68.517991
1127.612603	16.162840	68.522996
1126.867654	10.778052	68.528001
1126.232951	3.141223	68.533006
1125.420648	18.667785	68.538010
1124.420887	7.876809	68.543015
1123.482851	14.456944	68.548020
1123.051087	14.666179	68.553025
1122.581857	15.892185	68.558030
1122.296158	21.517023	68.563034
1122.071307	13.619461	68.568039
1120.700341	15.842014	68.573044
1120.292589	21.804805	68.578049
1119.695831	11.853310	68.583054
1118.488126	19.479270	68.588058
1117.931132	14.331090	68.593063
1117.417203	9.597102	68.598068
1117.055112	12.670000	68.603073
1115.831157	7.787178	68.608078
1115.065706	19.316658	68.613082
1114.827028	11.946415	68.618087
1114.296856	12.638075	68.623092
1113.652682	12.007478	68.628097
1112.747909	14.136960	68.633102
1112.074841	20.749071	68.638106
1111.903281	3.985419	68.643111
1110.973216	14.722653	68.648116
1109.782003	14.819303	68.653121
1109.706009	18.643046	68.658126
1108.722268	23.394911	68.663130
1108.419497	17.766332	68.668135
1107.273801	16.444390	68.673140
1106.741813	11.880432	68.678145
1106.554028	11.040049	68.683150
1105.223527	14.743219	68.688154
1104.574744	4.437316	68.693159
1103.801885	13.659347	68.698164
1103.325137	19.562152	68.703169
1103.054144	12.255397	68.708174
1102.886283	10.345842	68.713178
1102.313180	9.882135	68.718183
1101.189168	20.377417	68.723188
1100.236359	17.993484	68.728193
1099.305454	11.540741	68.733198
1098.442109	21.031058	68.738202
1098.308206	11.650911	68.743207
1097.857063	9.756454	68.748212
1097.345934	11.422785	68.753217
1096.178981	18.914539	68.758222
1095.501070	22.458718	68.763226
1095.371342	7.997039	68.768231
1093.894869	21.224438	68.773236
1093.196241	16.538758	68.778241
1093.119226	10.155193	68.783246
1092.629558	10.299528	68.788250
1092.434656	7.884926	68.793255
1091.209876	29.357487	68.798260
1090.659989	11.132274	68.803265
1089.850046	14.728992	68.808270
1088.574694	16.866968	68.813274
1088.361333	15.180690	68.818279
1088.106060	23.117201	68.823284
1086.966504	12.130862	68.828289
1086.016980	20.401730	68.833294
1085.358206	19.178959	68.838298
1085.372571	10.593657	68.843303
1084.622585	16.905775	68.848308
1083.445709	6.773767	68.853313
1083.064831	14.296598	68.858318
1082.278204	18.551922	68.863322
1082.071191	9.118755	68.868327
1080.987932	20.664104	68.873332
1080.108679	5.507963	68.878337
1079.741807	9.163511	68.883342
1079.188904	19.730376	68.888346
1079.020334	13.366106	68.893351
1077.850013	12.571636	68.898356
1077.434571	12.420319	68.903361
1077.021013	1.983971	68.908366
1075.460111	12.151367	68.913370
1074.725048	6.460680	68.918375
1074.445150	12.734289	68.923380
1074.091998	12.962565	68.928385
1073.211488	3.494617	68.933390
1072.292837	14.670008	68.938394
1072.297164	12.624255	68.943399
1071.419739	23.267977	68.948404
1070.443120	10.212028	68.953409
1069.979674	13.474516	68.958414
1069.511624	13.188068	68.963418
1068.798608	15.011098	68.968423
1067.507560	9.648550	68.973428
1066.912588	18.394446	68.978433
1066.433316	7.881819	68.983438
1066.264880	13.103232	68.988442
1065.092564	9.305035	68.993447
1064.320005	9.738801	68.998452
1063.968715	13.377681	69.003457
1063.542870	2.426058	69.008462
1062.547595	22.676257	69.013466
1062.024148	15.343437	69.018471
1061.453291	12.354719	69.023476
1061.051913	4.590909	69.028481
1059.904056	18.289584	69.033486
1058.989334	15.596838	69.038490
1058.809435	16.529251	69.043495
1058.213465	11.984945	69.048500
1057.001129	14.440913	69.053505
1056.562606	13.444883	69.058510
1056.060870	24.640693	69.063514
1055.688641	12.981955	69.068519
1054.549439	16.728833	69.073524
1053.553289	13.637465	69.078529
1053.379809	14.761242	69.083534
1052.933789	24.522645	69.088538
1052.296995	11.907799	69.093543
1051.251970	10.454753	69.098548
1050.839019	22.128439	69.103553
1050.549014	18.404348	69.108558
1049.260871	13.235309	69.113562
1048.671483	14.877829	69.118567
1048.302629	13.615255	69.123572
1047.794442	7.388598	69.128577
1046.779745	8.327661	69.133582
1045.843030	16.183345	69.138586
1045.961563	10.115601	69.143591
1044.950287	15.797523	69.148596
1043.870591	6.288735	69.153601
1043.568909	9.754147	69.158606
1042.756007	22.589003	69.163610
1041.932299	12.180061	69.168615
1041.014211	13.531104	69.173620
1040.725112	11.561995	69.178625
1040.415115	15.254231	69.183630
1039.564597	23.821596	69.188634
1038.919690	7.499111	69.193639
1038.195271	3.314288	69.198644
1037.560484	14.386181	69.203649
1037.378020	5.627199	69.208654
1036.173370	7.861182	69.213658
1035.938494	7.324760	69.218663
1034.832553	10.451351	69.223668
1033.581340	4.029098	69.228673
1033.055586	12.741907	69.233678
1032.687731	12.504180	69.238682
1032.334040	1.331357	69.243687
1032.062272	5.321857	69.248692
1031.227688	7.157928	69.253697
1030.464948	15.906864	69.258702
1029.518551	11.982858	69.263706
1028.825724	5.197387	69.268711
1028.148922	15.613657	69.273716
1027.788177	4.623301	69.278721
1027.311709	17.310015	69.283726
1026.151643	7.219520	69.288730
1025.585656	3.889422	69.293735
1024.730203	7.692090	69.298740
1024.325147	13.712805	69.303745
1023.844677	8.339593	69.308750
1022.799229	6.620126	69.313754
1022.173603	-2.273344	69.318759
1021.823937	-2.170193	69.323764
1020.947450	8.157996	69.328769
1020.174169	-1.079408	69.333774
1019.659606	13.658640	69.338778
1019.391499	2.853819	69.343783
1018.480189	9.639462	69.348788
1017.353024	2.426366	69.353793
1017.196302	0.513470	69.358798
1016.197073	8.070026	69.363802
1015.939103	-3.226827	69.368807
1014.898344	2.275291	69.373812
1013.864485	1.668872	69.378817
1013.631879	14.463441	69.383822
1013.177213	12.140637	69.388826
1012.773681	1.049864	69.393831
1011.722611	14.165457	69.398836
1010.870585	10.429868	69.403841
1010.490277	13.059405	69.408846
1009.833125	16.119336	69.413850
1009.517835	0.085047	69.418855
1008.468382	15.739238	69.423860
1008.013112	3.836693	69.428865
1006.939083	3.515784	69.433870
1006.360452	12.656471	69.438874
1006.028499	15.073315	69.443879
1005.885336	10.584714	69.448884
1004.825969	10.974244	69.453889
1003.888988	-1.376771	69.458894
1003.104057	15.230376	69.463898
1002.328211	-1.725675	69.468903
1001.348185	17.129674	69.473908
1000.834224	18.681358	69.478913
1000.619200	12.296106	69.483918
999.915439	21.682209	69.488922
999.699545	12.904894	69.493927
998.405873	13.744862	69.498932
997.813324	9.988494	69.503937
997.556610	15.410031	69.508942
996.471261	15.655468	69.513946
995.534181	19.013826	69.518951
995.115378	13.812155	69.523956
994.457103	15.591802	69.528961
994.363677	11.265597	69.533966
993.382063	14.046000	69.538970
992.497763	16.063456	69.543975
991.752971	7.846530	69.548980
991.366785	13.892630	69.553985
990.686427	10.788891	69.558990
989.993616	15.418812	69.563994
989.558291	17.330142	69.568999
988.540199	21.592357	69.574004
987.736270	18.845742	69.579009
987.377334	4.661828	69.584014
986.640007	19.831135	69.589018
986.228769	8.159704	69.594023
984.941663	11.622641	69.599028
984.569724	6.631135	69.604033
984.392946	10.409409	69.609038
983.480740	15.192510	69.614042
982.646273	18.536122	69.619047
981.878203	15.348571	69.624052
981.433843	13.661212	69.629057
981.042036	5.990513	69.634062
979.663139	19.889976	69.639066
978.984926	8.056025	69.644071
978.654330	15.943018	69.649076
978.078001	16.824974	69.654081
978.097281	10.684716	69.659086
976.829274	12.551921	69.664090
976.448260	7.730591	69.669095
975.552110	17.968887	69.674100
974.256008	20.362528	69.679105
974.002473	11.132322	69.684110
973.479624	15.169087	69.689114
973.164020	14.591900	69.694119
971.920123	9.701290	69.699124
971.245343	21.187984	69.704129
971.118926	16.753490	69.709134
970.546347	15.714152	69.714138
969.645348	9.225171	69.719143
968.651842	17.298068	69.724148
968.389609	10.123985	69.729153
967.667680	8.923912	69.734158
966.417637	12.183845	69.739162
965.865028	8.760171	69.744167
965.824744	8.098177	69.749172
965.048716	12.780767	69.754177
964.769390	1.198743	69.759182
963.855286	10.911623	69.764186
962.902614	11.626387	69.769191
961.903548	7.780176	69.774196
961.349605	15.686939	69.779201
961.054252	7.981973	69.784206
960.359987	16.280066	69.789210
959.518290	7.900378	69.794215
958.632415	14.492762	69.799220
958.034255	4.032205	69.804225
957.942438	-0.835136	69.809230
956.905630	11.721546	69.814234
956.036508	5.949732	69.819239
955.446876	14.757869	69.824244
955.060120	15.634896	69.829249
954.581746	12.407565	69.834254
953.471771	17.073914	69.839258
953.059457	7.805902	69.844263
952.422253	23.131170	69.849268
951.533518	12.472422	69.854273
950.807387	18.392851	69.859278
949.845824	19.725614	69.864282
949.758885	11.806138	69.869287
949.259981	15.586788	69.874292
948.573289	9.407484	69.879297
947.815892	8.900601	69.884302
947.009385	15.373128	69.889306
946.375998	13.821510	69.894311
945.423672	16.054807	69.899316
944.719702	15.667154	69.904321
944.609100	1.538356	69.909326
943.843361	23.601785	69.914330
943.370552	8.910884	69.919335
942.334122	9.925985	69.924340
941.516479	20.949723	69.929345
941.596607	11.693236	69.934350
940.231681	15.542310	69.939354
939.399109	12.704078	69.944359
938.821185	18.110501	69.949364
938.400691	7.694215	69.954369
938.073921	11.169935	69.959374
937.320592	10.154637	69.964378
936.595389	8.597132	69.969383
935.941743	8.121051	69.974388
935.010668	12.289013	69.979393
934.486469	6.224204	69.984398
933.914825	9.568583	69.989402
933.710250	3.599568	69.994407
932.322351	14.539010	69.999412
931.472409	8.399883	70.004417
931.342281	-1.490177	70.009422
930.827815	21.022111	70.014426
929.865325	4.795945	70.019431
929.109473	11.384992	70.024436
928.664082	16.469133	70.029441
928.244471	10.332489	70.034446
926.699105	13.130088	70.039450
926.430032	11.496847	70.044455
925.488962	12.968281	70.049460
925.314657	7.547950	70.054465
925.165363	10.624851	70.059470
923.780595	18.187601	70.064474
923.200486	10.302455	70.069479
922.726899	9.890763	70.074484
921.573088	13.326211	70.079489
921.352922	4.410825	70.084494
920.628475	17.301007	70.089498
920.639840	0.875722	70.094503
919.236375	12.096761	70.099508
918.163548	14.106397	70.104513
918.324970	5.984981	70.109518
917.698359	19.110327	70.114522
916.762171	3.379871	70.119527
915.631941	10.129420	70.124532
915.181136	9.258372	70.129537
915.004997	2.925296	70.134542
913.714581	18.605244	70.139546
913.163878	1.487250	70.144551
912.466610	11.608753	70.149556
912.045936	4.685398	70.154561
911.923516	14.690191	70.159566
910.606087	9.492778	70.164570
909.976098	8.615553	70.169575
909.757207	8.931294	70.174580
908.671260	9.903826	70.179585
907.971050	4.108306	70.184590
906.997512	17.239977	70.189594
907.030823	16.424349	70.194599
906.367565	18.357773	70.199604
905.166443	19.468483	70.204609
904.992238	0.948612	70.209614
904.312534	17.300912	70.214618
903.458577	6.997772	70.219623
902.714140	8.881037	70.224628
901.789435	8.687795	70.229633
902.008168	-0.330547	70.234638
900.493130	18.811812	70.239642
899.928021	3.813927	70.244647
899.691000	-1.154877	70.249652
899.011201	12.906161	70.254657
898.258764	-0.264210	70.259662
896.840734	9.871076	70.264666
896.667268	11.895285	70.269671
896.646656	9.288965	70.274676
895.722550	14.435102	70.279681
894.676788	9.112463	70.284686
894.188497	12.577624	70.289690
893.797215	11.299721	70.294695
892.940664	6.882089	70.299700
892.023681	6.840583	70.304705
891.654097	6.707230	70.309710
890.860925	15.123575	70.314714
890.235396	14.430146	70.319719
889.506764	10.410042	70.324724
888.739836	14.947704	70.329729
888.416332	5.613538	70.334734
887.629946	16.143463	70.339738
886.901306	1.024957	70.344743
886.390644	3.178522	70.349748
885.660859	23.198845	70.354753
885.116536	9.575886	70.359758
884.153188	16.789315	70.364762
883.411386	22.877832	70.369767
883.189631	16.466861	70.374772
882.366687	6.373257	70.379777
881.367006	6.210878	70.384782
880.571279	12.404166	70.389786
880.346791	11.377259	70.394791
879.955599	11.259961	70.399796
878.864023	7.518394	70.404801
878.398244	9.112894	70.409806
877.817253	17.702052	70.414810
877.611907	13.030975	70.419815
876.603787	4.684119	70.424820
875.813830	9.597603	70.429825
875.180695	8.167387	70.434830
873.860997	6.947364	70.439834
873.477298	9.725687	70.444839
873.161729	16.869139	70.449844
872.546148	9.265618	70.454849
871.810750	8.840411	70.459854
870.584946	10.710412	70.464858
870.415194	10.866950	70.469863
870.011666	5.369571	70.474868
868.877710	3.512873	70.479873
868.526776	4.278556	70.484878
867.874882	15.865696	70.489882
867.340813	17.113105	70.494887
866.625874	8.607628	70.499892
865.828118	14.295050	70.504897
865.220420	7.164933	70.509902
864.327331	12.627835	70.514906
863.672012	14.594697	70.519911
862.781198	6.117216	70.524916
862.417381	12.207074	70.529921
861.876106	16.366636	70.534926
861.638283	15.188891	70.539930
860.583137	9.027260	70.544935
859.876932	8.982180	70.549940
859.388095	10.990354	70.554945
858.592344	11.848912	70.559950
857.777769	18.978749	70.564954
857.092251	13.579867	70.569959
856.967360	13.798650	70.574964
855.954678	18.160974	70.579969
855.108095	3.332485	70.584974
854.094713	20.523210	70.589978
853.789062	5.905085	70.594983
853.589540	19.670501	70.599988
852.232075	17.876190	70.604993
851.855069	14.935519	70.609998
851.330099	19.802105	70.615002
851.000059	14.327723	70.620007
849.918811	10.745371	70.625012
849.129844	6.356422	70.630017
848.699657	12.291268	70.635022
848.159752	13.840802	70.640026
847.368969	10.980183	70.645031
846.640489	4.607298	70.650036
845.892843	18.623955	70.655041
845.653944	8.609292	70.660046
844.387838	3.898904	70.665050
843.506562	6.508851	70.670055
843.108801	9.085993	70.675060
842.719186	16.633886	70.680065
842.410852	9.831434	70.685070
841.392855	16.846997	70.690074
841.007884	18.602104	70.695079
840.251572	13.649727	70.700084
839.232813	11.334744	70.705089
838.467585	7.544406	70.710094
838.011942	16.246079	70.715098
837.446577	12.545351	70.720103
836.382606	19.421581	70.725108
835.958183	22.248971	70.730113
835.880699	18.666125	70.735118
835.294544	14.952938	70.740122
834.420348	8.778287	70.745127
833.931788	14.831235	70.750132
832.371016	18.486036	70.755137
831.745164	13.128127	70.760142
830.931434	16.129444	70.765146
830.681326	13.867156	70.770151
830.073186	18.773792	70.775156
829.691657	25.251247	70.780161
828.892020	6.301094	70.785166
827.859533	21.206749	70.790170
827.771115	10.092672	70.795175
827.290571	8.981950	70.800180
826.133627	20.244219	70.805185
825.623237	16.768128	70.810190
824.806190	24.232677	70.815194
824.138875	18.703175	70.820199
823.207044	10.957623	70.825204
822.278017	23.695889	70.830209
822.340208	11.852952	70.835214
821.988727	19.194508	70.840218
820.993543	26.488721	70.845223
820.314123	22.640573	70.850228
819.873269	19.535031	70.855233
819.012981	20.252490	70.860238
817.904925	24.300433	70.865242
817.185680	22.098629	70.870247
817.304043	14.764643	70.875252
816.253871	16.425368	70.880257
815.563332	11.535069	70.885262
814.496299	19.602372	70.890266
814.492306	7.907168	70.895271
813.969238	8.873720	70.900276
812.671700	17.625830	70.905281
812.229134	3.554629	70.910286
812.020615	14.970276	70.915290
811.302438	12.435574	70.920295
810.505393	15.063663	70.925300
809.247399	19.573861	70.930305
809.169240	18.894245	70.935310
808.029732	18.184883	70.940314
807.227224	16.141413	70.945319
806.936362	20.071894	70.950324
806.197127	17.964737	70.955329
806.418562	21.313785	70.960334
804.948307	23.646924	70.965338
804.609376	18.837850	70.970343
804.267166	13.436375	70.975348
802.993606	23.078792	70.980353
802.570040	22.911468	70.985358
801.787742	21.195937	70.990362
801.124655	19.321084	70.995367
800.030329	9.586099	71.000372
799.156314	24.494923	71.005377
799.084568	9.163075	71.010382
798.329101	31.095581	71.015386
798.249234	11.382745	71.020391
797.085038	18.555635	71.025396
796.064245	14.872222	71.030401
795.995581	6.613974	71.035406
795.122476	22.656461	71.040410
794.395174	12.453051	71.045415
793.931669	15.368667	71.050420
793.211394	27.280518	71.055425
792.649931	17.952709	71.060430
791.558232	29.676111	71.065434
791.149252	11.169977	71.070439
790.843360	19.387356	71.075444
789.768974	22.204679	71.080449
789.149993	8.588910	71.085454
788.374920	18.908901	71.090458
787.878334	17.598894	71.095463
787.545976	15.255089	71.100468
786.303169	8.819022	71.105473
785.763138	14.023899	71.110478
785.050065	16.942975	71.115482
784.558059	10.565581	71.120487
783.967061	12.675185	71.125492
782.850938	28.761097	71.130497
782.722283	13.160769	71.135502
782.180640	9.707011	71.140506
781.259053	22.100331	71.145511
780.599795	8.397939	71.150516
779.817485	19.870239	71.155521
779.786259	4.334834	71.160526
778.560448	21.068969	71.165530
777.859278	7.247098	71.170535
777.372981	13.268153	71.175540
776.564513	7.554565	71.180545
775.942572	13.964638	71.185550
775.013394	13.825769	71.190554
774.563489	14.771221	71.195559
774.379344	15.910904	71.200564
773.569844	22.292493	71.205569
772.757336	10.379079	71.210574
772.088807	13.876105	71.215578
771.242057	11.224692	71.220583
770.239924	13.546403	71.225588
769.430367	21.905465	71.230593
769.118606	13.137146	71.235598
768.910601	15.840206	71.240602
768.402603	10.922440	71.245607
767.486477	13.946384	71.250612
766.301026	15.417357	71.255617
766.412050	12.960394	71.260622
765.598486	16.303896	71.265626
764.875329	14.891194	71.270631
764.107863	12.041084	71.275636
763.379257	15.189716	71.280641
762.549995	7.747980	71.285646
761.708816	18.368653	71.290650
761.336832	8.203310	71.295655
761.150813	6.648329	71.300660
760.508069	21.826263	71.305665
759.809236	12.638606	71.310670
759.025343	13.097923	71.315674
757.874028	12.382579	71.320679
757.323921	12.639100	71.325684
756.376375	13.340510	71.330689
756.168390	8.010717	71.335694
755.799907	13.569904	71.340698
754.990528	3.873161	71.345703
754.447374	8.438307	71.350708
753.999863	7.713419	71.355713
753.058323	8.000719	71.360718
752.116651	14.674583	71.365722
751.907939	16.633448	71.370727
751.021909	2.027331	71.375732
749.778934	15.506279	71.380737
749.593153	12.380645	71.385742
748.985138	8.997386	71.390746
748.089828	20.834606	71.395751
747.496361	15.187720	71.400756
746.700660	12.025149	71.405761
746.598532	11.887083	71.410766
745.873028	14.803417	71.415770
744.870794	15.709077	71.420775
744.084394	10.830910	71.425780
743.503237	13.740033	71.430785
743.149524	14.268060	71.435790
741.648950	19.102331	71.440794
740.920268	7.106204	71.445799
740.536042	10.635243	71.450804
739.972294	10.663709	71.455809
740.012968	4.192062	71.460814
739.361188	20.238742	71.465818
738.155031	12.686711	71.470823
737.672371	19.588695	71.475828
736.846983	12.076967	71.480833
736.753472	17.425225	71.485838
735.681776	12.493136	71.490842
735.007965	18.711206	71.495847
734.633655	18.359436	71.500852
733.521678	16.420455	71.505857
732.793691	10.851761	71.510862
732.122479	14.388647	71.515866
731.674991	17.448377	71.520871
731.339335	16.606337	71.525876
730.593710	13.071530	71.530881
729.966528	10.446674	71.535886
729.071723	19.238778	71.540890
728.285361	11.973147	71.545895
727.767857	11.191600	71.550900
726.863475	17.220881	71.555905
726.751781	9.363721	71.560910
725.762070	19.922898	71.565914
724.949915	9.766144	71.570919
724.436389	14.094772	71.575924
723.851155	12.190201	71.580929
723.432458	5.020577	71.585934
721.875716	14.995108	71.590938
721.737545	4.027743	71.595943
721.499155	13.965835	71.600948
720.415666	12.262017	71.605953
719.613904	11.112575	71.610958
719.072511	11.990602	71.615962
718.940786	14.728828	71.620967
718.312734	1.152385	71.625972
716.872818	10.844969	71.630977
716.670324	8.407962	71.635982
716.102512	12.273734	71.640986
715.279826	11.985472	71.645991
714.384149	16.069024	71.650996
713.684894	14.061186	71.656001
713.690160	14.292369	71.661006
712.599945	12.991741	71.666010
712.020697	4.567221	71.671015
711.458821	10.586125	71.676020
710.796654	10.461537	71.681025
709.832462	8.469076	71.686030
709.168804	21.732806	71.691034
708.620486	15.872166	71.696039
707.688875	12.710749	71.701044
707.008332	13.282934	71.706049
706.584999	11.983358	71.711054
705.976979	5.197114	71.716058
705.605377	5.805263	71.721063
704.789724	8.545152	71.726068
703.655404	2.542861	71.731073
703.546896	7.182311	71.736078
702.480956	9.984129	71.741082
701.753299	11.580933	71.746087
700.651206	8.662702	71.751092
700.207400	13.711925	71.756097
700.120098	14.631193	71.761102
699.508453	15.851564	71.766106
699.167488	17.000452	71.771111
698.341316	13.505288	71.776116
697.549429	21.058899	71.781121
696.831427	1.890823	71.786126
695.610170	20.265834	71.791130
695.013469	12.460671	71.796135
694.816780	3.748168	71.801140
694.583048	14.109709	71.806145
693.872466	12.130489	71.811150
693.072875	11.635133	71.816154
692.115779	5.259282	71.821159
691.153217	8.412067	71.826164
690.205753	12.163257	71.831169
690.131845	5.146896	71.836174
689.699763	8.540060	71.841178
688.787377	14.731472	71.846183
688.180975	10.556358	71.851188
687.697529	13.978203	71.856193
686.848463	10.699574	71.861198
685.924551	19.564131	71.866202
685.033073	8.935910	71.871207
684.568562	2.210400	71.876212
684.163927	8.500731	71.881217
684.004257	2.999258	71.886222
683.112083	9.499681	71.891226
682.334252	14.414440	71.896231
681.912307	9.894572	71.901236
680.542244	10.658557	71.906241
679.433347	12.137879	71.911246
679.210587	9.620526	71.916250
678.985105	13.696719	71.921255
678.538986	10.008585	71.926260
677.344479	7.858850	71.931265
677.074513	5.248091	71.936270
676.367769	13.645991	71.941274
675.335040	3.500732	71.946279
674.682899	9.445706	71.951284
673.656373	12.148222	71.956289
673.761238	2.241283	71.961294
673.276155	9.455886	71.966298
672.639530	16.604739	71.971303
671.813300	8.504981	71.976308
670.907392	8.769293	71.981313
670.446039	-2.666980	71.986318
669.411904	-3.203825	71.991322
668.637020	-2.633954	71.996327
668.312098	-5.918765	72.001332
667.742129	1.523813	72.006337
667.423523	-5.152385	72.011342
666.510811	4.230769	72.016346
665.932899	-0.975448	72.021351
664.939503	8.430018	72.026356
663.915908	1.864502	72.031361
663.544279	1.455548	72.036366
663.324025	7.527289	72.041370
662.557721	2.559225	72.046375
661.681707	2.074473	72.051380
660.949911	5.335597	72.056385
660.309667	-4.168840	72.061390
659.945792	5.912227	72.066394
658.950951	1.523017	72.071399
658.532669	1.443184	72.076404
657.652845	0.596348	72.081409
657.161185	10.456498	72.086414
656.156469	2.539710	72.091418
655.550024	8.531027	72.096423
655.245376	5.443256	72.101428
654.544435	15.100197	72.106433
653.730410	3.493008	72.111438
653.047804	7.604147	72.116442
652.386832	3.634851	72.121447
652.202952	-0.930802	72.126452
651.104429	18.520634	72.131457
650.416932	2.898954	72.136462
649.860494	10.943345	72.141466
649.269698	11.785100	72.146471
648.358201	-2.709673	72.151476
647.511024	13.748161	72.156481
647.493892	2.231691	72.161486
646.712786	7.481285	72.166490
645.917128	2.686631	72.171495
645.357957	-7.324285	72.176500
644.817497	9.874738	72.181505
643.965001	1.093219	72.186510
642.886247	9.209748	72.191514
642.329443	10.446630	72.196519
642.377319	-5.739989	72.201524
640.964924	6.687355	72.206529
640.323342	3.058744	72.211534
639.673707	1.758950	72.216538
639.321968	0.943140	72.221543
639.212429	-6.359267	72.226548
637.626888	0.571698	72.231553
637.254852	-11.455934	72.236558
637.067695	-4.850161	72.241562
636.057576	1.820440	72.246567
635.218816	-0.531002	72.251572
634.712141	2.572856	72.256577
634.570365	-11.431056	72.261582
633.178281	-2.495095	72.266586
632.242546	-1.085906	72.271591
632.146531	-4.180089	72.276596
630.759174	14.912076	72.281601
630.102619	-4.223167	72.286606
629.409012	10.563906	72.291610
629.289852	-0.665081	72.296615
628.962518	-0.147547	72.301620
628.710615	5.818850	72.306625
627.902123	2.115900	72.311630
627.058657	6.971738	72.316634
625.779478	9.132624	72.321639
625.205642	-5.687138	72.326644
624.499109	6.504803	72.331649
624.264956	2.872812	72.336654
623.653562	5.469811	72.341658
622.435404	7.799172	72.346663
621.995268	-3.433887	72.351668
621.562191	3.029708	72.356673
621.132378	-5.323959	72.361678
619.856666	4.011362	72.366682
619.088633	2.039739	72.371687
618.925382	-4.087191	72.376692
618.196648	9.699401	72.381697
617.371050	3.621182	72.386702
616.613270	7.118264	72.391706
616.178198	5.522537	72.396711
615.708089	6.408156	72.401716
614.723283	9.528242	72.406721
614.129460	2.848574	72.411726
613.436803	3.977789	72.416730
612.974629	-0.974037	72.421735
612.100188	1.584434	72.426740
611.076136	7.432535	72.431745
611.060349	3.762615	72.436750
610.681932	-0.951820	72.441754
609.393694	5.296316	72.446759
608.812212	-7.704030	72.451764
607.866449	2.985360	72.456769
607.877136	-1.300620	72.461774
606.963921	4.515637	72.466778
606.095691	7.596660	72.471783
606.146350	-6.650783	72.476788
604.930191	2.764944	72.481793
604.359739	1.469896	72.486798
603.410431	4.000870	72.491802
602.874832	6.680419	72.496807
602.266012	5.525519	72.501812
601.264993	9.909728	72.506817
600.780593	5.376173	72.511822
600.213785	3.522315	72.516826
599.823335	7.213207	72.521831
599.057145	8.794098	72.526836
597.873484	6.090753	72.531841
597.454052	-4.300365	72.536846
597.271281	-0.555820	72.541850
596.413271	3.177998	72.546855
595.650744	-4.463520	72.551860
594.590556	0.789533	72.556865
594.662987	-8.192884	72.561870
593.582075	6.258489	72.566874
593.063627	2.755357	72.571879
592.316134	-6.657857	72.576884
591.702605	5.565006	72.581889
591.163335	-4.633563	72.586894
590.217057	4.554688	72.591898
589.728042	-2.799237	72.596903
589.515067	-2.637373	72.601908
588.360996	9.189047	72.606913
587.604681	-7.796708	72.611918
587.136533	-1.092565	72.616922
586.114546	9.318822	72.621927
585.915479	-4.180808	72.626932
584.472184	2.896262	72.631937
584.348619	-4.061713	72.636942
583.983634	-4.331368	72.641946
583.542156	-0.996617	72.646951
582.771752	-5.230729	72.651956
582.030689	7.785140	72.656961
581.395688	-4.153292	72.661966
580.502127	4.239683	72.666970
579.866168	8.572063	72.671975
579.293044	-5.788910	72.676980
577.959613	-7.118545	72.681985
577.315787	-6.889634	72.686990
576.988131	-1.991362	72.691994
576.144984	9.033350	72.696999
576.251670	-6.207010	72.702004
575.676405	1.208040	72.707009
574.701521	-7.792065	72.712014
574.200043	8.760521	72.717018
573.185636	5.366348	72.722023
572.254788	2.471366	72.727028
571.700605	7.583914	72.732033
571.498344	-2.274097	72.737038
570.543451	2.900695	72.742042
569.537232	16.756728	72.747047
569.156838	-8.227111	72.752052
568.312524	8.342234	72.757057
568.179978	2.677186	72.762062
567.311035	-0.185076	72.767066
566.402244	7.981677	72.772071
566.323077	0.409516	72.777076
565.480462	7.028232	72.782081
564.671068	5.269791	72.787086
563.649700	1.427310	72.792090
563.355009	-1.621031	72.797095
562.833953	-7.162694	72.802100
561.479932	4.446426	72.807105
561.352255	3.752631	72.812110
561.093853	2.483582	72.817114
560.336937	3.917931	72.822119
559.738450	-1.496285	72.827124
558.994759	7.055748	72.832129
558.324106	1.186258	72.837134
556.975432	4.761704	72.842138
556.567735	8.865348	72.847143
556.416169	-3.742998	72.852148
554.832206	8.442059	72.857153
554.318006	7.368293	72.862158
554.032560	-2.254120	72.867162
553.538613	9.170706	72.872167
553.251803	0.384277	72.877172
551.919577	5.023103	72.882177
551.357864	-5.469916	72.887182
550.618617	-1.113196	72.892186
549.753863	5.887511	72.897191
549.471989	1.971401	72.902196
548.169101	5.396059	72.907201
548.110416	0.116633	72.912206
547.776366	7.408115	72.917210
546.733495	-4.369143	72.922215
546.269011	-3.001871	72.927220
545.705970	4.591007	72.932225
545.086503	-8.412725	72.937230
544.016281	0.309588	72.942234
543.224586	5.240780	72.947239
543.079697	-5.123092	72.952244
542.282817	3.971991	72.957249
541.217055	-2.664016	72.962254
540.975700	4.838199	72.967258
540.669483	-2.875983	72.972263
539.856557	7.114194	72.977268
538.665085	3.469127	72.982273
538.314698	10.876752	72.987278
537.611776	4.712792	72.992282
536.401614	-0.189255	72.997287
535.935110	-8.043477	73.002292
535.361155	0.115675	73.007297
535.106364	0.853472	73.012302
534.627843	0.113065	73.017306
533.485071	-0.769110	73.022311
532.951294	-6.595737	73.027316
532.439667	0.894336	73.032321
531.595723	1.213481	73.037326
530.522109	6.604314	73.042330
530.189019	0.170141	73.047335
529.757376	-3.726838	73.052340
528.624783	4.701072	73.057345
527.777836	0.972747	73.062350
527.129228	-2.290443	73.067354
526.673301	5.950836	73.072359
526.543922	1.720285	73.077364
525.916023	0.393407	73.082369
525.574608	-2.041948	73.087374
524.850154	-3.848597	73.092378
523.583978	2.285677	73.097383
522.556224	3.660679	73.102388
522.071491	-4.868713	73.107393
521.703204	-1.110383	73.112398
521.408591	0.797525	73.117402
520.446235	-0.681074	73.122407
520.008996	-0.986517	73.127412
518.919541	11.279057	73.132417
518.494999	-0.856878	73.137422
517.340984	6.871145	73.142426
516.508749	-1.773198	73.147431
516.487600	-8.398978	73.152436
515.888669	-0.507074	73.157441
515.273241	-0.918170	73.162446
514.358621	-1.888718	73.167450
513.601787	-1.411559	73.172455
513.188832	-12.574792	73.177460
512.258339	5.593089	73.182465
511.642929	-5.921090	73.187470
511.023353	2.448757	73.192474
510.368150	0.670503	73.197479
510.224673	-1.909920	73.202484
509.162689	0.918152	73.207489
508.376613	-2.353095	73.212494
507.702362	2.548359	73.217498
507.187241	4.377857	73.222503
506.679071	-0.621809	73.227508
505.551979	1.000832	73.232513
505.005963	-4.610955	73.237518
504.866311	4.287977	73.242522
504.142248	4.524958	73.247527
503.409513	-5.524493	73.252532
502.751205	6.090516	73.257537
501.739249	-2.662383	73.262542
501.181973	-7.222146	73.267546
500.440575	9.444354	73.272551
500.370581	-2.096787	73.277556
499.095864	7.462350	73.282561
498.369577	0.018517	73.287566
497.700015	4.056652	73.292570
497.266762	1.525546	73.297575
496.558752	-0.299483	73.302580
495.689130	-0.195427	73.307585
495.975704	-0.742326	73.312590
495.097381	-3.480066	73.317594
494.144443	-2.910161	73.322599
493.832351	-1.556118	73.327604
492.449490	5.471949	73.332609
491.729534	2.054560	73.337614
491.093772	-0.674513	73.342618
490.669441	-1.893466	73.347623
490.072923	4.980948	73.352628
489.029830	2.859226	73.357633
488.401880	10.509763	73.362638
488.260840	0.574206	73.367642
487.296221	9.051066	73.372647
486.269443	-9.126277	73.377652
485.380792	11.280479	73.382657
484.958485	-1.609568	73.387662
484.547391	1.805511	73.392666
484.032448	8.433548	73.397671
483.964641	-5.173700	73.402676
482.636788	9.913122	73.407681
482.201835	12.497814	73.412686
481.465808	7.619606	73.417690
480.129384	13.533288	73.422695
479.832090	-1.319438	73.427700
478.864398	3.273964	73.432705
478.849859	0.209389	73.437710
478.569035	8.495315	73.442714
477.977776	1.316977	73.447719
477.152418	2.355408	73.452724
476.423249	5.625624	73.457729
475.126000	7.745308	73.462734
474.871773	1.637620	73.467738
473.959960	15.328828	73.472743
473.725200	1.923211	73.477748
472.119280	11.861549	73.482753
471.645438	14.236401	73.487758
471.437887	3.999210	73.492762
470.922215	16.739504	73.497767
470.580189	-1.818160	73.502772
469.362217	10.966209	73.507777
468.875191	-6.122313	73.512782
468.332179	4.903487	73.517786
467.444472	4.330783	73.522791
466.738387	5.993598	73.527796
466.335035	-1.003365	73.532801
465.599605	4.443997	73.537806
464.744471	-6.000668	73.542810
463.711376	1.686032	73.547815
463.352644	-2.626240	73.552820
462.793720	5.416992	73.557825
462.623546	3.913130	73.562830
461.867190	-3.286205	73.567834
460.700404	13.433884	73.572839
460.486067	6.107191	73.577844
459.692689	4.470810	73.582849
459.017203	1.751229	73.587854
458.568549	3.019803	73.592858
457.536816	6.249920	73.597863
456.816268	1.549025	73.602868
456.124868	2.006315	73.607873
455.730729	-4.105884	73.612878
455.443163	3.372156	73.617882
454.072676	5.812595	73.622887
453.774037	4.184125	73.627892
453.229083	4.684314	73.632897
451.915715	-1.718238	73.637902
451.373353	3.494944	73.642906
450.914365	14.296060	73.647911
450.665253	-3.188325	73.652916
449.969545	0.144373	73.657921
448.878792	-2.024930	73.662926
448.363846	2.348119	73.667930
447.520028	3.280694	73.672935
447.654635	1.070700	73.677940
446.482252	6.732761	73.682945
445.640204	0.070619	73.687950
444.930745	2.088784	73.692954
444.418775	-1.721264	73.697959
443.473587	6.143822	73.702964
442.637515	5.249094	73.707969
442.476381	3.647601	73.712974
442.200310	3.612954	73.717978
440.716758	9.923825	73.722983
440.225960	6.108826	73.727988
439.557659	-1.183377	73.732993
439.378350	3.803233	73.737998
438.664262	5.489407	73.743002
437.628108	9.486620	73.748007
437.151786	-2.685192	73.753012
436.843147	9.662575	73.758017
435.976715	12.919981	73.763022
435.080767	9.134842	73.768026
434.360475	9.163089	73.773031
434.156934	-0.896538	73.778036
432.957822	10.930804	73.783041
432.259127	6.603317	73.788046
431.263568	14.496937	73.793050
430.809189	6.092036	73.798055
430.943211	-0.187888	73.803060
429.880528	10.816644	73.808065
429.227014	3.384894	73.813070
428.719056	0.982397	73.818074
427.848070	8.753667	73.823079
426.942628	-1.517391	73.828084
426.050067	1.985446	73.833089
425.817756	4.722357	73.838094
425.603093	1.675478	73.843098
424.982582	13.295519	73.848103
424.358011	3.954242	73.853108
423.555319	11.826594	73.858113
422.395269	13.911830	73.863118
421.837090	6.294583	73.868122
421.153432	7.621108	73.873127
420.983170	0.169133	73.878132
419.959236	3.114176	73.883137
418.747488	2.233585	73.888142
418.681724	2.843505	73.893146
417.988048	5.816351	73.898151
417.640656	4.228769	73.903156
416.300548	9.296263	73.908161
415.916950	-1.513668	73.913166
415.667355	4.021871	73.918170
414.676370	8.869737	73.923175
414.095067	7.991193	73.928180
413.426190	10.398707	73.933185
412.863129	6.538460	73.938190
412.450933	5.798548	73.943194
411.340150	13.491341	73.948199
410.832444	10.811269	73.953204
409.559683	8.836561	73.958209
408.574650	3.502904	73.963214
408.598429	-2.149186	73.968218
408.031239	6.440985	73.973223
407.704966	0.008905	73.978228
407.397847	1.527742	73.983233
406.498657	5.411680	73.988238
406.061073	3.731241	73.993242
404.606371	17.464817	73.998247
403.886736	3.190326	74.003252
403.083298	27.166293	74.008257
402.843539	4.279475	74.013262
402.461797	6.737431	74.018266
401.181423	18.883661	74.023271
400.710339	12.532997	74.028276
399.881473	12.215864	74.033281
399.694044	9.867952	74.038286
398.923314	11.435433	74.043290
398.010775	17.147574	74.048295
397.834823	3.576489	74.053300
396.865970	4.666196	74.058305
396.022609	5.400024	74.063310
395.355661	7.485543	74.068314
394.679143	5.592449	74.073319
394.596914	1.594090	74.078324
393.495552	6.327091	74.083329
392.696699	6.199138	74.088334
392.401620	3.083077	74.093338
391.818191	5.574748	74.098343
390.887505	4.352924	74.103348
390.132902	14.832150	74.108353
389.578440	5.487597	74.113358
388.942388	1.473412	74.118362
387.762064	12.555051	74.123367
387.318497	0.318111	74.128372
386.774528	3.432684	74.133377
386.585969	-5.799860	74.138382
386.169929	-1.824176	74.143386
384.759193	5.996843	74.148391
384.690408	1.352960	74.153396
383.491210	10.283539	74.158401
382.496198	-1.816641	74.163406
382.448013	9.150820	74.168410
381.693270	8.825035	74.173415
381.198302	7.964280	74.178420
379.982076	3.314014	74.183425
379.610780	-6.259984	74.188430
379.086341	-5.581703	74.193434
378.397572	6.284176	74.198439
378.032538	-4.145510	74.203444
376.885938	4.037112	74.208449
376.487979	5.303929	74.213454
376.203774	3.017172	74.218458
374.560856	3.019000	74.223463
374.150407	-3.885348	74.228468
373.613867	11.464915	74.233473
373.211475	2.214405	74.238478
372.638409	6.380692	74.243482
371.728189	7.618756	74.248487
371.633858	3.497751	74.253492
370.476308	6.177108	74.258497
369.515484	0.331845	74.263502
368.928338	4.910373	74.268506
368.587748	7.997273	74.273511
367.965606	2.772959	74.278516
367.037572	6.410777	74.283521
366.317029	6.144200	74.288526
366.161239	3.980481	74.293530
364.751159	8.664921	74.298535
364.099371	7.729814	74.303540
363.490441	2.232167	74.308545
363.219221	1.256915	74.313550
363.004948	5.165757	74.318554
361.538022	4.865164	74.323559
360.792855	-2.397416	74.328564
360.427312	8.961230	74.333569
360.208058	10.568570	74.338574
359.480113	6.789805	74.343578
358.629117	3.435919	74.348583
358.283610	-3.234352	74.353588
357.171106	8.979749	74.358593
356.355386	5.172397	74.363598
355.943828	7.426957	74.368602
355.344388	9.780843	74.373607
354.897073	-2.769293	74.378612
353.663561	6.816452	74.383617
353.271540	-0.808326	74.388622
352.665600	-4.601798	74.393626
351.950434	5.582570	74.398631
351.056527	5.723662	74.403636
350.577255	3.426996	74.408641
350.053934	1.353387	74.413646
348.900207	3.451839	74.418650
348.160954	10.741678	74.423655
348.090904	-10.432803	74.428660
347.579910	-5.300298	74.433665
346.882128	-2.937047	74.438670
345.931527	-1.839192	74.443674
345.111240	-3.550089	74.448679
344.832642	-3.144363	74.453684
343.970246	-2.632984	74.458689
343.037421	-5.033980	74.463694
342.481265	-9.046689	74.468698
342.102789	4.737734	74.473703
341.899771	-12.050649	74.478708
340.644565	4.719825	74.483713
339.922004	1.569399	74.488718
339.533973	-7.110964	74.493722
338.836260	7.528563	74.498727
337.876908	-5.126039	74.503732
337.226968	9.816530	74.508737
336.590930	1.235610	74.513742
336.338086	5.759290	74.518746
335.378834	7.760525	74.523751
334.854056	-6.794132	74.528756
334.385447	3.171175	74.533761
333.262372	-4.015397	74.538766
332.479909	-0.099578	74.543770
332.002366	8.635586	74.548775
331.800664	3.426277	74.553780
331.017046	12.799989	74.558785
330.177338	17.253203	74.563790
329.739766	6.082894	74.568794
328.962081	11.412449	74.573799
328.133681	-3.711970	74.578804
327.327416	7.984991	74.583809
326.812921	9.921654	74.588814
326.583804	6.850282	74.593818
325.204197	11.569310	74.598823
324.880266	14.216754	74.603828
324.337501	7.272001	74.608833
323.500756	-0.089508	74.613838
322.484039	7.834322	74.618842
321.635505	2.341760	74.623847
321.652072	3.905210	74.628852
320.984797	7.050487	74.633857
320.863557	6.809833	74.638862
319.407050	4.976419	74.643866
318.791050	5.576268	74.648871
318.579057	9.833249	74.653876
317.256169	11.253795	74.658881
316.666137	9.469939	74.663886
316.055583	4.300563	74.668890
315.551958	12.000700	74.673895
315.360175	-3.272483	74.678900
314.196495	6.973914	74.683905
313.497478	4.084666	74.688910
313.357795	-3.916200	74.693914
311.782283	-0.189363	74.698919
311.223673	-1.516188	74.703924
310.724849	0.168827	74.708929
310.458714	5.199240	74.713934
310.257511	1.748116	74.718938
308.930359	3.598266	74.723943
308.721364	-2.820946	74.728948
308.036707	9.518942	74.733953
306.826603	5.230430	74.738958
306.245431	1.175985	74.743962
305.587065	10.644853	74.748967
305.292266	1.243176	74.753972
303.960374	6.656336	74.758977
303.235470	4.895557	74.763982
303.173298	-1.080288	74.768986
302.643820	2.765257	74.773991
302.502900	0.351598	74.778996
301.512623	7.862800	74.784001
300.887677	2.441840	74.789006
300.133253	-3.821053	74.794010
298.929593	9.325360	74.799015
298.440070	-1.779884	74.804020
297.268779	5.444786	74.809025
296.524270	-1.032571	74.814030
296.550534	3.072896	74.819034
295.882373	8.984230	74.824039
295.278014	-6.656837	74.829044
294.159278	3.481478	74.834049
293.839324	3.911147	74.839054
293.443936	0.429477	74.844058
292.488404	0.958872	74.849063
292.059383	-0.811216	74.854068
291.026677	5.844179	74.859073
290.516490	1.466196	74.864078
289.944606	9.306521	74.869082
288.774946	8.015595	74.874087
288.296138	6.590903	74.879092
287.934234	5.344691	74.884097
287.394473	3.931291	74.889102
286.418403	6.094492	74.894106
285.356459	9.097686	74.899111
285.164291	5.558393	74.904116
284.677730	13.437160	74.909121
283.845783	2.881648	74.914126
283.169162	3.238861	74.919130
282.498651	9.117457	74.924135
282.275885	5.160429	74.929140
281.506601	9.261816	74.934145
280.269632	7.877547	74.939150
279.633086	-0.747424	74.944154
279.071478	6.367460	74.949159
278.661364	0.641036	74.954164
278.185037	7.824327	74.959169
277.130944	11.343500	74.964174
276.753215	9.497431	74.969178
276.277075	11.483183	74.974183
275.055205	5.763147	74.979188
274.226185	14.256306	74.984193
273.610879	9.198083	74.989198
273.467508	3.157912	74.994202
272.754874	17.533337	74.999207
272.057351	5.324294	75.004212
271.676147	12.460888	75.009217
270.908881	11.134215	75.014222
270.106168	4.429606	75.019226
269.106763	13.826689	75.024231
268.694956	7.018771	75.029236
268.130998	14.069381	75.034241
267.286449	7.992745	75.039246
266.742398	13.206230	75.044250
266.288017	15.516514	75.049255
265.431777	6.243758	75.054260
264.195261	14.248377	75.059265
263.437025	7.924600	75.064270
263.264340	4.462628	75.069274
262.657378	16.384877	75.074279
262.415648	12.897639	75.079284
261.872960	14.845117	75.084289
260.998457	19.743858	75.089294
260.174440	9.710624	75.094298
259.040303	15.316207	75.099303
258.204536	0.945182	75.104308
257.500498	9.804764	75.109313
257.313368	11.006455	75.114318
257.170309	14.369378	75.119322
256.479176	11.070469	75.124327
256.062324	15.659723	75.129332
255.102587	20.505822	75.134337
254.530304	11.946301	75.139342
253.335411	2.585612	75.144346
252.350546	9.838932	75.149351
252.367594	8.198014	75.154356
251.719244	15.202157	75.159361
250.829516	5.111596	75.164366
250.136311	7.464682	75.169370
249.817379	11.431214	75.174375
249.355953	12.195670	75.179380
248.079028	12.721123	75.184385
247.018652	10.121304	75.189390
246.985832	6.490384	75.194394
246.395940	8.663003	75.199399
245.828274	14.089986	75.204404
245.019450	3.336845	75.209409
244.374967	13.152009	75.214414
244.061956	5.708621	75.219418
242.826817	16.852667	75.224423
242.546570	7.775102	75.229428
241.723458	10.084245	75.234433
240.826874	10.484418	75.239438
240.372966	-0.095066	75.244442
239.699943	13.610165	75.249447
238.986954	6.640535	75.254452
238.117662	6.334632	75.259457
236.977978	9.553659	75.264462
237.084755	14.731209	75.269466
236.216589	11.507834	75.274471
236.179591	8.057349	75.279476
235.194764	12.983144	75.284481
234.444538	7.083869	75.289486
233.910997	7.653248	75.294490
232.709404	12.421215	75.299495
232.100803	13.499288	75.304500
231.488922	15.856761	75.309505
230.768656	21.211884	75.314510
230.640003	18.789965	75.319514
229.726532	16.584617	75.324519
229.502461	8.586170	75.329524
228.664714	13.501136	75.334529
227.934439	5.736347	75.339534
227.351907	0.578302	75.344538
226.304887	6.300892	75.349543
225.597651	3.031370	75.354548
224.722058	8.714018	75.359553
223.894682	13.960061	75.364558
223.825188	-0.552024	75.369562
223.068103	7.732562	75.374567
222.901738	-0.301885	75.379572
221.501668	8.747507	75.384577
220.967502	5.420434	75.389582
220.777414	1.336784	75.394586
219.780748	10.835943	75.399591
219.174452	2.359130	75.404596
218.522695	11.077925	75.409601
218.209104	0.914461	75.414606
217.413748	6.932817	75.419610
216.024780	7.864068	75.424615
215.980361	5.821375	75.429620
215.647468	8.914948	75.434625
214.247187	6.094949	75.439630
213.665935	10.164802	75.444634
212.835309	11.825464	75.449639
212.620515	9.505587	75.454644
212.459443	8.238410	75.459649
211.207485	14.547176	75.464654
210.879718	1.277875	75.469658
210.020119	14.869355	75.474663
208.785310	6.303511	75.479668
208.290890	11.745631	75.484673
207.718113	11.627428	75.489678
207.739975	10.067742	75.494682
206.844948	12.150247	75.499687
205.926974	7.173413	75.504692
205.477829	10.479481	75.509697
205.035448	14.615505	75.514702
204.178030	-3.342671	75.519706
203.081240	11.619112	75.524711
202.839172	0.198487	75.529716
201.899992	8.934721	75.534721
201.165651	18.631761	75.539726
200.899062	-1.158368	75.544730
200.020809	16.184411	75.549735
199.450156	11.672588	75.554740
198.516011	5.433651	75.559745
197.728237	3.834313	75.564750
197.410698	3.421538	75.569754
197.003931	1.624267	75.574759
196.205393	13.886138	75.579764
195.221122	7.344541	75.584769
195.010699	11.981313	75.589774
193.972043	7.878411	75.594778
192.917197	17.244936	75.599783
192.403315	6.739676	75.604788
192.277116	10.502026	75.609793
191.770227	7.859722	75.614798
190.969051	14.323706	75.619802
190.196431	13.207643	75.624807
189.838412	6.485783	75.629812
188.642981	14.826074	75.634817
187.931979	4.035285	75.639822
187.383705	11.219020	75.644826
186.838653	13.523272	75.649831
186.365442	5.408441	75.654836
185.342442	8.446465	75.659841
184.825313	11.517377	75.664846
184.347536	-0.740851	75.669850
183.117443	6.059589	75.674855
182.424397	5.017572	75.679860
181.947983	3.010640	75.684865
181.646719	11.214680	75.689870
181.585373	4.081258	75.694874
180.066893	14.810041	75.699879
179.646128	4.775631	75.704884
179.179944	3.277988	75.709889
177.967557	4.237876	75.714894
177.257692	1.654746	75.719898
176.240672	5.581198	75.724903
176.222047	2.616631	75.729908
176.146640	5.719617	75.734913
175.015792	12.352856	75.739918
174.473004	11.304232	75.744922
173.658245	8.980670	75.749927
172.926980	11.792418	75.754932
172.153091	6.609704	75.759937
171.492329	10.868857	75.764942
171.371912	12.052032	75.769946
170.147368	10.626416	75.774951
169.293841	10.494638	75.779956
168.907830	5.675851	75.784961
168.506564	12.899227	75.789966
167.804324	12.372755	75.794970
166.833899	13.469108	75.799975
166.238986	12.720526	75.804980
166.088989	15.672983	75.809985
164.761568	13.968889	75.814990
164.490295	6.312287	75.819994
163.324477	15.646053	75.824999
163.201236	11.277366	75.830004
162.739478	16.693785	75.835009
161.783376	12.136199	75.840014
161.679692	7.660319	75.845018
160.284758	22.209203	75.850023
159.543811	15.201479	75.855028
158.930379	14.268198	75.860033
158.089002	11.829039	75.865038
157.969583	10.287149	75.870042
156.704671	18.551803	75.875047
156.149635	9.114378	75.880052
155.798665	13.994329	75.885057
155.291433	15.776908	75.890062
154.745734	10.652431	75.895066
153.794616	13.392008	75.900071
152.913994	16.342692	75.905076
152.575177	1.592870	75.910081
151.762710	9.533075	75.915086
150.917429	10.617365	75.920090
150.262131	21.519191	75.925095
150.233550	15.195806	75.930100
149.027311	14.623546	75.935105
148.138341	25.351326	75.940110
147.383510	16.114487	75.945114
147.315262	14.543938	75.950119
146.939580	11.393458	75.955124
146.241298	12.424351	75.960129
145.354969	8.107954	75.965134
144.904037	7.055729	75.970138
143.275801	8.835704	75.975143
142.790888	18.691676	75.980148
142.457364	10.721734	75.985153
141.734986	12.628503	75.990158
141.758076	5.505275	75.995162
140.625138	18.209977	76.000167
139.970295	8.820011	76.005172
139.301396	17.043252	76.010177
138.429501	17.986715	76.015182
137.524175	6.868970	76.020186
136.839446	12.037100	76.025191
136.681766	13.152103	76.030196
136.275675	3.236789	76.035201
135.420119	13.891429	76.040206
134.740345	9.110027	76.045210
134.058654	7.236758	76.050215
133.125911	3.269959	76.055220
132.300122	3.289886	76.060225
131.552051	7.315393	76.065230
131.474879	4.521008	76.070234
131.073802	7.940844	76.075239
130.148810	3.331007	76.080244
129.504644	2.438903	76.085249
128.696101	16.946331	76.090254
128.370122	7.437701	76.095258
127.186722	6.999002	76.100263
126.600694	7.816463	76.105268
126.085610	6.908509	76.110273
125.276292	11.552473	76.115278
124.384731	6.771731	76.120282
123.841011	17.289921	76.125287
123.308662	6.894859	76.130292
123.108269	8.803553	76.135297
122.317128	12.988892	76.140302
121.567323	6.200214	76.145306
120.600053	14.100459	76.150311
120.075788	0.085100	76.155316
119.451098	12.800222	76.160321
119.042995	17.082176	76.165326
118.802748	4.374515	76.170330
117.287647	12.303771	76.175335
116.728488	5.678655	76.180340
116.084263	4.977372	76.185345
115.508330	12.707986	76.190350
114.263643	11.848568	76.195354
113.363608	11.413575	76.200359
113.187105	11.579125	76.205364
112.855542	11.819863	76.210369
112.604874	5.080903	76.215374
112.240755	9.153998	76.220378
111.227445	4.529867	76.225383
110.304109	17.295770	76.230388
109.238497	8.324545	76.235393
108.415915	9.859382	76.240398
108.453090	3.522366	76.245402
107.717724	19.241814	76.250407
106.849432	6.437190	76.255412
106.201480	8.995980	76.260417
105.156379	9.574423	76.265422
105.146827	0.258190	76.270426
104.226849	9.231081	76.275431
102.980677	0.947807	76.280436
102.529913	6.007672	76.285441
102.200670	4.004096	76.290446
101.921664	8.265463	76.295450
101.267558	9.119017	76.300455
100.333450	12.491397	76.305460
100.075353	8.439105	76.310465
98.968036	13.603671	76.315470
98.286831	6.357796	76.320474
97.346912	7.501350	76.325479
96.887202	18.767796	76.330484
96.506205	7.907071	76.335489
95.363921	8.310210	76.340494
95.141925	9.818660	76.345498
94.629455	8.825143	76.350503
93.908602	8.820464	76.355508
92.887827	14.490036	76.360513
92.067001	13.520461	76.365518
91.755576	11.607082	76.370522
91.105968	10.641742	76.375527
90.311076	3.589038	76.380532
89.614103	4.321701	76.385537
89.103359	13.040109	76.390542
88.622945	11.459600	76.395546
87.373103	17.567817	76.400551
86.751882	11.736330	76.405556
86.677296	8.753883	76.410561
85.959233	8.275688	76.415566
85.036380	0.905935	76.420570
84.194542	23.241743	76.425575
83.985446	15.069047	76.430580
83.447639	5.814978	76.435585
82.342853	13.500628	76.440590
81.706799	11.739942	76.445594
80.834681	11.141241	76.450599
80.565611	17.626050	76.455604
79.695165	7.130383	76.460609
78.614801	18.429578	76.465614
78.761859	4.176288	76.470618
77.807293	4.364999	76.475623
77.498241	12.431517	76.480628
76.431269	8.385224	76.485633
76.069795	17.207561	76.490638
75.278637	3.406661	76.495642
74.245086	8.985238	76.500647
73.368414	10.445135	76.505652
73.430019	10.102796	76.510657
72.948761	14.806419	76.515662
72.002328	12.573276	76.520666
70.919775	12.533249	76.525671
70.646739	22.599861	76.530676
70.165409	13.906049	76.535681
68.926069	22.805313	76.540686
68.840392	4.683127	76.545690
67.889868	8.692053	76.550695
67.054696	3.881843	76.555700
66.306479	8.689539	76.560705
65.482728	13.633858	76.565710
65.512607	7.271200	76.570714
64.803857	17.441988	76.575719
63.880501	11.061044	76.580724
63.471986	11.310906	76.585729
62.664262	11.665435	76.590734
62.343576	5.453301	76.595738
60.906279	2.188302	76.600743
60.699771	7.362179	76.605748
60.205580	4.689498	76.610753
59.111280	12.762981	76.615758
58.695053	-3.549796	76.620762
57.790567	4.564372	76.625767
57.414596	-2.674971	76.630772
57.025449	-2.240544	76.635777
55.837446	11.414377	76.640782
55.467167	2.934672	76.645786
54.810823	6.300613	76.650791
54.096213	5.771417	76.655796
53.388656	-6.667730	76.660801
52.199171	10.511821	76.665806
52.017915	-4.119594	76.670810
51.787144	8.338747	76.675815
50.882244	6.089529	76.680820
50.124014	7.771811	76.685825
49.365860	8.116862	76.690830
49.066095	3.440459	76.695834
47.691978	15.284815	76.700839
47.533768	1.387715	76.705844
46.955943	6.292815	76.710849
45.930131	5.398526	76.715854
45.484056	-1.266677	76.720858
44.669486	8.397451	76.725863
43.975658	8.418438	76.730868
43.770683	-4.668549	76.735873
42.838620	10.971885	76.740878
42.239293	3.014402	76.745882
41.599230	1.476712	76.750887
40.997170	6.270565	76.755892
40.050928	2.867338	76.760897
39.390922	9.441304	76.765902
39.125420	3.275566	76.770906
38.163259	10.493795	76.775911
37.796130	-0.224043	76.780916
37.415988	0.172682	76.785921
35.798450	9.882880	76.790926
35.237090	-2.708886	76.795930
34.387739	10.593994	76.800935
34.157376	4.045770	76.805940
33.857571	1.941318	76.810945
33.035208	6.317736	76.815950
32.135438	2.637449	76.820954
31.774240	8.766377	76.825959
31.127573	-2.349986	76.830964
30.171718	7.691484	76.835969
29.286441	14.033309	76.840974
28.944706	4.200797	76.845978
28.735066	-1.779887	76.850983
27.673344	12.627590	76.855988
27.185502	-1.932846	76.860993
26.472842	9.556863	76.865998
25.631489	-3.919041	76.871002
24.472748	5.150297	76.876007
24.064051	0.947002	76.881012
23.559182	-1.310816	76.886017
23.074069	5.823443	76.891022
22.500653	6.667302	76.896026
21.336580	4.196089	76.901031
20.988264	3.138560	76.906036
20.533299	5.158823	76.911041
19.566831	-0.551340	76.916046
18.796501	-1.150484	76.921050
18.359674	5.346887	76.926055
17.754286	5.514621	76.931060
17.629660	-2.685718	76.936065
16.429897	-1.395036	76.941070
15.654165	8.676054	76.946074
15.188117	-1.973961	76.951079
14.562280	2.167693	76.956084
13.628968	4.038757	76.961089
13.075039	11.053113	76.966094
12.611488	2.777524	76.971098
11.318499	2.859396	76.976103
10.773760	2.107581	76.981108
10.491267	-6.485455	76.986113
10.165868	8.154650	76.991118
9.126624	-10.040906	76.996122
8.006227	-9.701141	77.001127
7.842624	-6.749666	77.006132
7.637398	-0.935770	77.011137
6.466338	-2.450253	77.016142
5.929998	-4.838661	77.021147
5.140896	4.696836	77.026151
4.344921	3.765905	77.031156
3.662964	-5.275909	77.036161