Mon Mar 08 18:07:54 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.221679	90.316480	0.000000
-0.358216	101.316953	0.005005
-1.294740	68.788116	0.010010
-2.527904	17.632911	0.015014
-5.417266	-18.100752	0.020019
-10.510976	-25.907441	0.025024
-16.480634	-16.982220	0.030029
-21.431019	-27.552405	0.035034
-25.147173	-32.169526	0.040038
-29.195301	-22.513180	0.045043
-32.661738	-29.294211	0.050048
-36.398221	-12.451152	0.055053
-40.067572	-23.470063	0.060058
-43.619230	-22.283587	0.065062
-47.647766	-15.657987	0.070067
-51.227189	-21.217793	0.075072
-55.381763	-14.852763	0.080077
-58.998139	-20.592738	0.085082
-62.264319	-17.677759	0.090086
-66.035788	-19.002883	0.095091
-69.707589	-18.907343	0.100096
-73.764441	-23.419578	0.105101
-77.561471	-22.348445	0.110106
-81.435325	-29.950625	0.115110
-85.254097	-22.612558	0.120115
-88.836926	-32.500354	0.125120
-92.604112	-17.052615	0.130125
-96.594525	-25.391513	0.135130
-100.116023	-28.292365	0.140134
-104.127449	-16.721088	0.145139
-107.472080	-27.042663	0.150144
-111.520191	-20.924756	0.155149
-115.424170	-25.546462	0.160154
-118.883790	-20.777648	0.165158
-122.955569	-8.950711	0.170163
-126.447208	-25.329341	0.175168
-130.659809	-14.569566	0.180173
-134.048682	-20.648488	0.185178
-137.405064	-26.729432	0.190182
-141.410829	-23.229582	0.195187
-145.172436	-36.034411	0.200192
-149.336275	-28.289543	0.205197
-153.284503	-26.738443	0.210202
-156.685456	-32.028525	0.215206
-161.096050	-16.760291	0.220211
-164.594408	-25.086125	0.225216
-167.979144	-26.278839	0.230221
-171.840284	-17.172482	0.235226
-175.261814	-31.040747	0.240230
-179.196770	-22.641669	0.245235
-182.864755	-23.506898	0.250240
-186.894614	-19.418099	0.255245
-190.524184	-26.631739	0.260250
-194.325684	-25.909783	0.265254
-198.128545	-19.275804	0.270259
-201.700998	-30.365099	0.275264
-205.620943	-25.101675	0.280269
-209.558675	-20.920312	0.285274
-212.879043	-23.419447	0.290278
-216.972524	-24.557330	0.295283
-220.619657	-30.870862	0.300288
-224.568256	-19.348852	0.305293
-228.201804	-25.071627	0.310298
-231.916795	-29.885719	0.315302
-235.656298	-19.474084	0.320307
-239.275936	-32.314030	0.325312
-243.163714	-25.018328	0.330317
-246.831554	-25.820406	0.335322
-250.630239	-21.962358	0.340326
-254.881647	-21.125923	0.345331
-258.388995	-31.621565	0.350336
-262.164938	-26.152386	0.355341
-265.911535	-26.970249	0.360346
-269.282681	-30.043073	0.365350
-273.044033	-21.679444	0.370355
-276.820865	-26.477286	0.375360
-280.541838	-32.376827	0.380365
-284.479725	-28.198476	0.385370
-288.478844	-31.587339	0.390374
-292.556139	-16.860925	0.395379
-296.049725	-28.273308	0.400384
-299.822232	-25.124237	0.405389
-303.937388	-29.715070	0.410394
-307.193170	-29.578346	0.415398
-311.115755	-17.942089	0.420403
-314.424501	-27.983663	0.425408
-318.338112	-25.936367	0.430413
-322.066573	-29.710565	0.435418
-325.824730	-32.448725	0.440422
-329.611599	-18.478222	0.445427
-333.749511	-22.693225	0.450432
-337.580107	-26.675014	0.455437
-341.009186	-24.919490	0.460442
-344.571085	-31.322122	0.465446
-348.609431	-12.897706	0.470451
-352.194878	-28.639689	0.475456
-356.185275	-26.143274	0.480461
-359.868705	-26.655694	0.485466
-363.433209	-41.798612	0.490470
-367.365695	-30.958608	0.495475
-371.205327	-22.188113	0.500480
-374.990178	-28.867329	0.505485
-378.901685	-23.556096	0.510490
-382.595742	-32.709753	0.515494
-386.502490	-14.661095	0.520499
-389.980599	-40.770891	0.525504
-393.517449	-21.832000	0.530509
-397.282920	-28.711386	0.535514
-400.757905	-28.490652	0.540518
-404.864712	-24.936396	0.545523
-408.714977	-32.660054	0.550528
-412.593538	-27.954826	0.555533
-416.613689	-30.209478	0.560538
-419.933494	-36.537109	0.565542
-423.937409	-21.407492	0.570547
-427.347656	-37.364965	0.575552
-431.381735	-23.941453	0.580557
-435.186766	-24.305034	0.585562
-438.736610	-34.008309	0.590566
-442.630183	-23.556008	0.595571
-446.275737	-31.187716	0.600576
-450.194230	-20.587925	0.605581
-454.007148	-35.093388	0.610586
-457.629524	-34.505273	0.615590
-461.449691	-18.104000	0.620595
-465.226474	-30.540024	0.625600
-468.861763	-38.062949	0.630605
-472.922340	-22.919480	0.635610
-476.341338	-27.316842	0.640614
-480.322159	-22.494255	0.645619
-483.890532	-37.729396	0.650624
-487.730031	-22.684286	0.655629
-491.550481	-25.311313	0.660634
-495.225681	-27.534192	0.665638
-499.132174	-29.187135	0.670643
-502.851204	-17.299256	0.675648
-506.520834	-29.919473	0.680653
-510.444290	-33.496652	0.685658
-514.283817	-23.327254	0.690662
-517.968306	-22.727550	0.695667
-521.374732	-32.117721	0.700672
-525.058578	-33.405649	0.705677
-529.388463	-33.350950	0.710682
-532.812226	-28.248259	0.715686
-536.830796	-24.753604	0.720691
-540.677847	-28.907465	0.725696
-544.176030	-21.925828	0.730701
-547.998392	-28.895222	0.735706
-551.434848	-28.276739	0.740710
-555.473457	-35.131155	0.745715
-558.745039	-30.789145	0.750720
-562.998277	-21.589609	0.755725
-566.889823	-20.742298	0.760730
-570.497790	-34.714189	0.765734
-574.145274	-25.351209	0.770739
-578.223812	-23.215649	0.775744
-582.070642	-30.710912	0.780749
-585.721380	-25.702773	0.785754
-589.159515	-21.006121	0.790758
-593.329368	-27.771702	0.795763
-596.697694	-39.260375	0.800768
-600.271267	-33.135488	0.805773
-604.184152	-19.029349	0.810778
-608.084719	-23.406353	0.815782
-612.052723	-25.695809	0.820787
-615.792750	-35.731102	0.825792
-619.492166	-28.874904	0.830797
-623.300778	-27.589760	0.835802
-626.610404	-26.557785	0.840806
-631.056459	-25.009947	0.845811
-634.662230	-33.445613	0.850816
-638.163938	-28.237288	0.855821
-641.988403	-26.538012	0.860826
-645.592999	-30.172214	0.865830
-649.471608	-32.893763	0.870835
-653.086562	-32.737028	0.875840
-657.100254	-22.356668	0.880845
-660.840461	-27.670646	0.885850
-664.629802	-34.157857	0.890854
-668.190819	-24.624061	0.895859
-672.296018	-31.324134	0.900864
-675.696156	-35.448254	0.905869
-679.417077	-23.935125	0.910874
-683.196073	-37.925227	0.915878
-687.383891	-21.367124	0.920883
-690.821716	-32.549673	0.925888
-694.520641	-21.923095	0.930893
-698.267330	-32.859167	0.935898
-702.032501	-32.731969	0.940902
-706.078674	-29.456542	0.945907
-709.560873	-26.400533	0.950912
-713.374645	-32.771799	0.955917
-717.313966	-32.012799	0.960922
-721.015623	-38.075550	0.965926
-724.918075	-30.511842	0.970931
-728.444640	-40.085909	0.975936
-732.116411	-35.963559	0.980941
-736.021837	-24.600630	0.985946
-739.972040	-30.722978	0.990950
-744.035193	-27.990378	0.995955
-747.154949	-27.718679	1.000960
-750.981113	-29.481807	1.005965
-754.604793	-22.730546	1.010970
-758.379514	-36.140905	1.015974
-762.395823	-25.323164	1.020979
-766.060626	-16.838618	1.025984
-769.968899	-22.789430	1.030989
-773.754338	-24.152192	1.035994
-777.441583	-39.787294	1.040998
-781.357397	-30.114640	1.046003
-784.778292	-17.906591	1.051008
-788.644648	-26.658318	1.056013
-792.534184	-33.077263	1.061018
-796.224282	-30.128245	1.066022
-800.378499	-27.108192	1.071027
-803.435741	-31.547116	1.076032
-807.405063	-17.728106	1.081037
-810.537336	-26.653895	1.086042
-813.979514	-29.843881	1.091046
-818.427538	-30.047302	1.096051
-822.500891	-28.807829	1.101056
-826.341967	-25.284296	1.106061
-830.476201	-15.646027	1.111066
-833.904227	-27.247796	1.116070
-837.545431	-25.758843	1.121075
-841.081570	-31.942471	1.126080
-844.891661	-22.028003	1.131085
-849.435626	-21.686196	1.136090
-852.566272	-20.513790	1.141094
-856.759649	-16.383556	1.146099
-860.187388	-27.340381	1.151104
-863.625265	-31.336769	1.156109
-867.701985	-22.792536	1.161114
-871.342816	-42.359765	1.166118
-875.108332	-25.386352	1.171123
-878.685418	-32.608851	1.176128
-883.016543	-22.234154	1.181133
-886.564756	-24.057265	1.186138
-890.088885	-34.158146	1.191142
-894.145193	-32.065025	1.196147
-897.953173	-31.470219	1.201152
-901.312179	-27.746106	1.206157
-904.971579	-29.904634	1.211162
-908.619271	-22.802393	1.216166
-912.930496	-25.165766	1.221171
-916.334807	-25.389221	1.226176
-920.121712	-25.214047	1.231181
-924.170290	-21.174654	1.236186
-927.862238	-30.341935	1.241190
-931.867902	-25.080997	1.246195
-935.813280	-29.248435	1.251200
-939.559201	-32.960498	1.256205
-943.364533	-19.664221	1.261210
-946.426748	-30.835463	1.266214
-950.194023	-26.106178	1.271219
-953.949100	-32.369733	1.276224
-958.158714	-31.464615	1.281229
-962.219723	-27.468901	1.286234
-965.432549	-29.239867	1.291238
-969.424485	-27.117489	1.296243
-972.583871	-36.418733	1.301248
-976.288107	-39.445147	1.306253
-980.334734	-17.338018	1.311258
-984.343553	-32.810961	1.316262
-987.888961	-34.561826	1.321267
-992.044342	-38.518970	1.326272
-995.566021	-39.319602	1.331277
-999.468819	-25.734860	1.336282
-1003.006416	-26.482476	1.341286
-1006.962794	-22.791989	1.346291
-1010.818971	-29.332583	1.351296
-1014.390381	-38.091654	1.356301
-1018.285576	-38.799403	1.361306
-1021.906644	-35.378551	1.366310
-1025.875389	-20.580055	1.371315
-1029.512578	-28.965903	1.376320
-1033.254750	-32.908638	1.381325
-1037.049585	-22.699866	1.386330
-1040.553090	-24.750654	1.391334
-1044.541734	-27.657360	1.396339
-1048.148681	-32.298181	1.401344
-1051.846299	-27.352807	1.406349
-1055.668020	-20.641965	1.411354
-1059.114326	-24.493215	1.416358
-1063.269256	-26.778807	1.421363
-1067.034725	-29.229182	1.426368
-1070.900440	-30.701617	1.431373
-1074.789915	-24.014601	1.436378
-1078.552690	-30.022838	1.441382
-1081.930554	-29.409802	1.446387
-1085.285556	-27.967824	1.451392
-1089.489074	-34.503181	1.456397
-1093.556099	-28.361722	1.461402
-1097.321269	-29.884887	1.466406
-1101.258457	-21.531314	1.471411
-1104.881497	-28.545835	1.476416
-1108.319646	-29.302891	1.481421
-1112.145591	-26.982907	1.486426
-1115.701458	-35.424194	1.491430
-1119.493114	-25.036042	1.496435
-1123.404569	-24.168862	1.501440
-1127.322489	-27.935101	1.506445
-1131.372716	-30.768729	1.511450
-1134.861582	-31.514477	1.516454
-1138.581010	-21.306576	1.521459
-1142.094185	-20.230279	1.526464
-1145.735037	-30.119695	1.531469
-1149.551070	-25.254571	1.536474
-1153.420229	-32.254867	1.541478
-1157.562382	-29.671342	1.546483
-1161.545228	-18.664358	1.551488
-1164.939563	-17.700076	1.556493
-1168.411879	-32.362835	1.561498
-1171.592832	-36.677390	1.566502
-1176.158741	-22.938979	1.571507
-1180.171577	-27.678646	1.576512
-1183.766910	-24.509235	1.581517
-1187.697434	-22.129819	1.586522
-1191.050685	-32.431010	1.591526
-1194.808351	-28.697893	1.596531
-1198.386566	-26.482058	1.601536
-1202.272907	-27.058458	1.606541
-1206.418258	-22.041206	1.611546
-1209.964121	-26.959613	1.616550
-1213.907373	-35.685669	1.621555
-1217.559197	-35.504819	1.626560
-1220.888835	-30.466687	1.631565
-1224.950613	-19.711889	1.636570
-1228.776222	-30.738495	1.641574
-1232.458990	-28.034391	1.646579
-1236.296979	-30.903370	1.651584
-1240.389269	-30.342933	1.656589
-1244.394720	-27.317528	1.661594
-1247.605987	-32.642637	1.666598
-1251.018847	-29.256331	1.671603
-1255.056118	-23.731190	1.676608
-1258.840282	-35.319433	1.681613
-1262.394769	-27.337494	1.686618
-1266.383495	-26.681625	1.691622
-1270.280792	-22.036681	1.696627
-1273.958216	-26.784129	1.701632
-1277.511418	-32.259468	1.706637
-1281.524777	-30.035367	1.711642
-1284.979661	-38.192930	1.716646
-1288.840878	-31.382370	1.721651
-1292.806269	-23.443428	1.726656
-1296.340720	-27.322783	1.731661
-1300.452636	-22.001651	1.736666
-1303.784783	-26.826386	1.741670
-1307.789332	-29.367403	1.746675
-1311.490287	-32.040578	1.751680
-1315.338484	-36.413709	1.756685
-1319.197880	-33.364248	1.761690
-1322.720229	-39.847344	1.766694
-1326.377085	-29.627107	1.771699
-1330.145515	-32.571713	1.776704
-1333.596935	-35.410942	1.781709
-1338.101004	-24.917890	1.786714
-1341.592306	-30.212233	1.791718
-1345.603271	-27.258310	1.796723
-1349.235157	-28.321448	1.801728
-1352.685283	-33.530904	1.806733
-1357.002629	-19.235887	1.811738
-1360.170468	-36.102655	1.816742
-1364.208797	-26.026291	1.821747
-1368.102472	-24.644330	1.826752
-1371.475085	-34.677221	1.831757
-1375.745984	-31.426184	1.836762
-1379.365842	-25.064101	1.841766
-1382.960409	-31.340012	1.846771
-1386.865686	-34.576415	1.851776
-1390.232336	-28.560766	1.856781
-1394.386143	-19.456141	1.861786
-1397.742682	-32.096571	1.866790
-1401.417481	-25.362978	1.871795
-1405.786783	-33.058587	1.876800
-1409.285850	-22.473995	1.881805
-1413.201823	-27.682894	1.886810
-1416.548262	-31.764038	1.891814
-1420.485614	-33.389986	1.896819
-1424.893383	-23.087225	1.901824
-1428.234525	-31.068819	1.906829
-1431.826100	-27.571642	1.911834
-1435.443382	-29.914251	1.916838
-1439.365925	-28.767234	1.921843
-1443.304027	-29.368053	1.926848
-1446.875237	-26.908545	1.931853
-1450.636172	-23.494604	1.936858
-1454.300471	-37.572658	1.941862
-1458.062330	-22.697816	1.946867
-1462.218295	-22.656623	1.951872
-1465.619985	-22.381397	1.956877
-1470.172389	-16.385496	1.961882
-1472.937101	-26.337383	1.966886
-1476.859368	-25.015313	1.971891
-1480.592670	-22.007852	1.976896
-1484.292252	-31.061009	1.981901
-1488.172154	-24.165137	1.986906
-1492.283442	-34.421738	1.991910
-1496.612703	-21.405000	1.996915
-1500.334312	-23.528658	2.006912
-1500.939287	-33.080003	2.016909
-1497.896101	-26.354515	2.026906
-1494.798118	-27.161232	2.036902
-1492.812363	-28.992964	2.046899
-1491.335243	-29.737490	2.056896
-1489.532422	-27.878468	2.066893
-1487.580487	-29.406368	2.076890
-1486.010874	-27.939459	2.086886
-1483.991099	-26.388321	2.096883
-1481.582274	-31.830829	2.106880
-1480.175321	-26.981138	2.116877
-1478.134208	-24.784485	2.126874
-1476.010929	-29.080776	2.136870
-1474.194945	-26.153357	2.146867
-1472.181233	-30.931030	2.156864
-1470.605110	-34.167104	2.166861
-1468.888120	-25.838217	2.176858
-1466.483976	-29.822640	2.186854
-1464.450749	-26.279493	2.196851
-1462.863421	-29.316837	2.206848
-1461.285133	-34.438453	2.216845
-1459.550420	-21.145187	2.226842
-1457.390125	-31.180361	2.236838
-1455.171818	-29.329417	2.246835
-1453.106606	-38.695695	2.256832
-1451.579070	-33.622145	2.266829
-1450.081378	-29.519571	2.276826
-1448.180789	-33.795970	2.286822
-1445.894212	-31.749112	2.296819
-1443.867750	-27.172265	2.306816
-1442.104368	-31.403008	2.316813
-1440.507679	-27.513639	2.326810
-1438.631184	-29.117838	2.336806
-1436.266142	-37.434776	2.346803
-1434.719028	-37.380499	2.356800
-1432.742393	-37.314466	2.366797
-1431.118071	-32.534282	2.376794
-1429.001577	-28.977592	2.386790
-1426.852649	-38.013054	2.396787
-1425.265805	-39.588236	2.406784
-1423.633624	-29.537371	2.416781
-1421.566204	-29.288500	2.426778
-1419.763846	-27.617236	2.436774
-1417.610428	-32.265657	2.446771
-1415.908429	-30.518325	2.456768
-1414.027337	-26.358688	2.466765
-1411.684149	-23.965606	2.476762
-1410.186248	-24.313948	2.486758
-1408.262689	-25.965130	2.496755
-1406.546528	-28.448344	2.506752
-1404.145692	-25.586078	2.516749
-1402.446230	-34.315889	2.526746
-1401.745478	-31.238294	2.536742
-1399.689501	-30.131810	2.546739
-1397.237025	-25.004191	2.556736
-1394.836005	-29.447502	2.566733
-1393.177469	-24.647501	2.576730
-1391.623126	-24.996971	2.586726
-1389.419755	-31.581198	2.596723
-1387.593805	-22.357082	2.606720
-1385.731272	-24.713718	2.616717
-1383.770854	-22.009865	2.626714
-1382.131529	-28.034861	2.636710
-1379.907227	-24.703796	2.646707
-1378.425143	-27.275831	2.656704
-1376.702201	-27.238609	2.666701
-1374.589599	-27.326919	2.676698
-1372.638581	-22.284783	2.686694
-1370.540700	-31.605705	2.696691
-1368.774403	-27.719750	2.706688
-1366.848399	-33.321692	2.716685
-1365.214215	-30.001937	2.726682
-1363.332536	-23.128224	2.736678
-1361.522416	-29.499483	2.746675
-1359.320738	-30.276227	2.756672
-1357.671468	-35.058625	2.766669
-1355.614634	-23.188891	2.776666
-1353.892708	-32.086474	2.786662
-1352.116459	-25.879540	2.796659
-1350.043899	-29.176054	2.806656
-1348.173509	-34.063311	2.816653
-1346.622127	-32.724436	2.826650
-1344.597300	-29.291936	2.836646
-1342.672911	-23.358171	2.846643
-1340.815831	-35.907264	2.856640
-1338.479237	-31.165231	2.866637
-1336.816559	-29.062609	2.876634
-1335.265569	-34.219249	2.886630
-1333.063812	-34.410209	2.896627
-1331.034911	-34.380875	2.906624
-1329.497545	-34.612327	2.916621
-1327.837871	-25.341019	2.926618
-1325.648834	-26.755161	2.936614
-1323.983913	-31.443730	2.946611
-1321.804222	-30.770648	2.956608
-1320.057009	-26.137938	2.966605
-1318.348675	-27.091462	2.976602
-1316.297947	-25.677756	2.986598
-1314.304641	-33.396680	2.996595
-1312.597827	-35.579918	3.006592
-1310.546575	-32.380557	3.016589
-1308.860782	-33.076264	3.026586
-1307.176468	-42.454092	3.036582
-1305.191907	-36.703608	3.046579
-1302.932406	-32.252347	3.056576
-1301.249037	-33.989733	3.066573
-1299.361329	-31.127334	3.076570
-1297.483752	-34.790478	3.086566
-1295.738646	-38.625044	3.096563
-1293.835722	-30.681023	3.106560
-1291.936922	-28.622473	3.116557
-1290.278157	-29.389628	3.126554
-1288.094070	-35.700687	3.136550
-1285.982150	-40.996012	3.146547
-1284.267578	-33.642347	3.156544
-1282.408346	-27.432847	3.166541
-1280.634193	-26.243259	3.176538
-1278.997863	-31.762460	3.186534
-1277.071251	-32.526683	3.196531
-1274.875338	-35.699192	3.206528
-1273.141662	-36.353591	3.216525
-1271.397193	-25.308493	3.226522
-1269.260766	-27.115205	3.236518
-1267.681408	-30.130620	3.246515
-1265.634430	-27.860505	3.256512
-1263.795005	-31.414890	3.266509
-1261.542593	-30.917594	3.276506
-1260.092257	-28.321474	3.286502
-1257.938567	-31.626155	3.296499
-1256.365851	-28.017016	3.306496
-1254.492525	-34.003588	3.316493
-1252.583410	-27.173642	3.326490
-1250.643778	-33.646070	3.336486
-1248.920758	-31.043054	3.346483
-1246.764466	-35.563894	3.356480
-1245.148461	-32.762178	3.366477
-1242.966442	-29.869461	3.376474
-1241.171851	-36.866549	3.386470
-1239.420874	-38.657340	3.396467
-1237.487040	-39.689520	3.406464
-1235.469645	-35.704697	3.416461
-1233.797476	-38.586524	3.426458
-1231.926889	-35.036087	3.436454
-1229.699807	-34.277346	3.446451
-1227.998761	-38.149023	3.456448
-1226.196866	-29.081966	3.466445
-1224.597664	-32.097370	3.476442
-1222.648060	-27.433811	3.486438
-1220.475971	-34.486554	3.496435
-1218.890161	-34.158860	3.506432
-1216.814546	-36.288940	3.516429
-1214.852226	-29.993249	3.526426
-1213.012317	-31.929300	3.536422
-1211.198753	-41.431957	3.546419
-1209.191156	-32.923574	3.556416
-1207.241714	-31.305675	3.566413
-1205.915373	-32.423779	3.576410
-1203.806549	-34.579688	3.586406
-1201.494068	-30.836253	3.596403
-1199.911558	-32.454801	3.606400
-1198.133794	-33.739864	3.616397
-1196.417137	-38.678196	3.626394
-1194.459656	-33.093797	3.636390
-1192.267730	-35.337200	3.646387
-1190.590650	-39.907627	3.656384
-1188.821555	-32.731549	3.666381
-1186.719425	-27.964471	3.676378
-1184.701377	-31.037391	3.686374
-1182.822950	-34.594797	3.696371
-1181.224394	-38.228998	3.706368
-1179.608419	-37.752950	3.716365
-1177.496245	-35.780547	3.726362
-1175.346761	-42.745949	3.736358
-1173.905592	-34.492687	3.746355
-1171.927638	-41.110127	3.756352
-1169.582955	-32.846684	3.766349
-1168.104256	-30.158729	3.776346
-1166.185202	-32.724757	3.786342
-1164.638024	-32.553471	3.796339
-1162.215183	-37.664759	3.806336
-1160.194516	-30.697847	3.816333
-1158.726884	-30.580145	3.826330
-1157.031024	-30.009496	3.836326
-1155.040047	-34.011190	3.846323
-1153.180650	-28.786839	3.856320
-1151.086442	-28.175706	3.866317
-1149.404772	-24.236563	3.876314
-1147.283203	-29.629631	3.886310
-1145.420814	-29.982431	3.896307
-1143.462044	-32.456903	3.906304
-1141.764962	-24.890324	3.916301
-1140.188220	-32.476160	3.926298
-1137.866023	-28.257384	3.936294
-1136.026168	-32.054893	3.946291
-1134.166268	-32.042559	3.956288
-1132.250306	-32.793908	3.966285
-1130.856664	-35.913731	3.976282
-1128.740082	-34.494603	3.986278
-1126.836974	-31.497157	3.996275
-1124.836990	-33.785581	4.006272
-1122.926439	-35.879701	4.016269
-1121.160107	-29.161004	4.026266
-1119.116589	-22.886106	4.036262
-1117.396801	-29.710097	4.046259
-1115.563530	-29.174030	4.056256
-1113.794437	-27.700880	4.066253
-1111.622464	-25.622720	4.076250
-1109.754255	-27.893210	4.086246
-1107.842284	-24.474019	4.096243
-1106.036400	-29.796028	4.106240
-1104.448457	-28.063374	4.116237
-1102.330114	-23.758268	4.126234
-1100.750442	-25.278406	4.136230
-1098.629474	-27.295643	4.146227
-1096.815164	-26.889156	4.156224
-1094.833452	-26.381553	4.166221
-1093.026801	-24.044419	4.176218
-1091.167429	-24.704579	4.186214
-1089.199729	-26.007311	4.196211
-1087.337476	-24.847454	4.206208
-1085.337268	-28.962672	4.216205
-1083.471629	-32.846369	4.226202
-1081.697398	-21.393770	4.236198
-1079.875992	-25.268811	4.246195
-1077.961567	-28.535062	4.256192
-1076.223750	-28.886829	4.266189
-1074.216730	-18.657212	4.276186
-1072.318192	-27.000251	4.286182
-1070.392316	-26.703164	4.296179
-1068.579477	-31.989944	4.306176
-1066.779294	-30.259632	4.316173
-1064.810740	-32.277723	4.326170
-1063.025940	-24.238809	4.336166
-1060.899347	-26.493748	4.346163
-1058.989900	-25.440887	4.356160
-1057.299342	-30.655998	4.366157
-1055.578435	-31.796075	4.376154
-1053.879570	-32.444744	4.386150
-1051.734797	-26.628071	4.396147
-1049.925237	-28.979132	4.406144
-1047.891263	-23.564721	4.416141
-1046.042812	-27.409327	4.426138
-1044.050932	-25.231249	4.436134
-1042.178213	-23.053057	4.446131
-1040.526985	-24.466182	4.456128
-1038.762995	-27.081518	4.466125
-1036.619102	-23.200424	4.476122
-1034.694329	-28.945597	4.486118
-1033.027329	-29.701257	4.496115
-1030.902962	-29.034841	4.506112
-1029.388434	-33.002866	4.516109
-1027.706330	-26.027468	4.526106
-1025.317619	-29.121642	4.536102
-1023.342608	-33.839078	4.546099
-1021.512505	-38.628071	4.556096
-1019.592979	-29.972792	4.566093
-1017.934382	-28.677680	4.576090
-1016.434466	-28.576104	4.586086
-1014.105572	-28.591312	4.596083
-1012.218707	-25.201181	4.606080
-1010.434864	-32.886374	4.616077
-1008.602355	-21.509344	4.626074
-1006.715810	-23.610587	4.636070
-1004.949224	-33.105599	4.646067
-1002.804803	-30.370843	4.656064
-1001.152190	-26.998503	4.666061
-999.192235	-27.860987	4.676058
-997.195911	-26.409874	4.686054
-995.648035	-26.582789	4.696051
-993.206556	-23.259229	4.706048
-991.469360	-22.117189	4.716045
-989.761678	-23.829826	4.726042
-988.139758	-26.183992	4.736038
-986.088136	-26.462718	4.746035
-983.878375	-24.578369	4.756032
-982.385070	-30.938171	4.766029
-980.533584	-25.718721	4.776026
-978.473556	-23.895684	4.786022
-976.769734	-28.039207	4.796019
-974.761526	-22.080623	4.806016
-972.882561	-20.478094	4.816013
-971.073025	-24.741147	4.826010
-969.204705	-24.019521	4.836006
-967.414677	-26.727388	4.846003
-965.178404	-20.562111	4.856000
-963.299073	-20.518013	4.865997
-961.808177	-20.418117	4.875994
-959.511874	-19.586502	4.885990
-958.051881	-23.878915	4.895987
-956.039763	-16.067301	4.905984
-953.900023	-15.968520	4.915981
-952.336737	-17.926456	4.925978
-950.555662	-23.801744	4.935974
-948.695602	-32.084857	4.945971
-946.760364	-28.456097	4.955968
-944.655906	-21.066597	4.965965
-942.630229	-20.040119	4.975962
-940.962388	-19.005369	4.985958
-939.289413	-25.714395	4.995955
-937.267077	-21.940082	5.005952
-935.281402	-22.410320	5.015949
-933.504693	-23.748700	5.025946
-931.721839	-20.927644	5.035942
-929.947873	-25.363397	5.045939
-927.442896	-27.163994	5.055936
-925.891933	-28.275227	5.065933
-924.103018	-25.924070	5.075930
-922.485173	-20.828262	5.085926
-920.309892	-26.084468	5.095923
-918.389497	-26.177949	5.105920
-916.555983	-30.168486	5.115917
-914.624598	-23.618106	5.125914
-912.740748	-26.839867	5.135910
-911.090091	-23.601354	5.145907
-909.129026	-25.248658	5.155904
-906.978883	-28.715089	5.165901
-905.381883	-28.351077	5.175898
-903.456824	-25.394844	5.185894
-901.572339	-30.547700	5.195891
-899.866553	-31.213155	5.205888
-898.124315	-29.656600	5.215885
-895.925031	-21.781699	5.225882
-894.050720	-23.568275	5.235878
-892.256531	-26.080967	5.245875
-890.264438	-24.210675	5.255872
-888.463462	-29.596481	5.265869
-886.704449	-21.453821	5.275866
-884.533482	-20.466309	5.285862
-882.799256	-24.777258	5.295859
-880.918139	-34.137345	5.305856
-879.068395	-31.352205	5.315853
-877.120285	-27.281770	5.325850
-875.261465	-16.172499	5.335846
-873.598634	-30.637031	5.345843
-871.692726	-26.034068	5.355840
-869.560692	-31.649621	5.365837
-867.831937	-20.030092	5.375834
-865.970581	-29.661743	5.385830
-863.920341	-24.840273	5.395827
-862.066260	-22.141072	5.405824
-860.621296	-21.515888	5.415821
-858.422218	-24.559059	5.425818
-856.572387	-17.742962	5.435814
-854.622759	-25.224036	5.445811
-852.712194	-26.023242	5.455808
-850.709073	-31.363968	5.465805
-848.878572	-25.640538	5.475802
-847.308524	-30.992558	5.485798
-845.473044	-22.961559	5.495795
-843.556528	-20.346531	5.505792
-841.671723	-25.860966	5.515789
-839.597998	-15.695465	5.525786
-837.632477	-15.085584	5.535782
-835.840150	-28.236620	5.545779
-834.134435	-20.120132	5.555776
-832.151927	-26.786990	5.565773
-830.049165	-20.046037	5.575770
-828.668757	-23.727249	5.585766
-826.514334	-23.055977	5.595763
-824.701067	-17.582395	5.605760
-822.731913	-23.350293	5.615757
-820.932375	-21.441268	5.625754
-819.189957	-22.180413	5.635750
-816.952550	-29.649036	5.645747
-815.171639	-29.952237	5.655744
-813.462898	-27.221872	5.665741
-811.869570	-25.620923	5.675738
-809.542877	-25.147694	5.685734
-807.787954	-25.037798	5.695731
-805.836201	-18.713200	5.705728
-803.900808	-30.346066	5.715725
-802.159416	-30.399789	5.725722
-800.307887	-24.910200	5.735718
-798.150714	-27.678205	5.745715
-796.540981	-21.298933	5.755712
-794.507466	-27.337615	5.765709
-793.207846	-26.624424	5.775706
-791.136579	-26.205086	5.785702
-788.975284	-26.422225	5.795699
-786.891921	-22.217015	5.805696
-785.254982	-27.499165	5.815693
-783.525656	-17.442771	5.825690
-781.527002	-21.702758	5.835686
-779.696446	-18.216590	5.845683
-777.516559	-25.522834	5.855680
-775.750209	-24.937910	5.865677
-774.181819	-14.183170	5.875674
-771.953908	-21.964443	5.885670
-770.150213	-21.593900	5.895667
-768.569294	-28.494940	5.905664
-766.420015	-19.710358	5.915661
-764.717466	-27.393449	5.925658
-762.897900	-28.902759	5.935654
-760.893133	-24.812856	5.945651
-758.957252	-19.030403	5.955648
-757.033180	-25.885229	5.965645
-755.174881	-23.541870	5.975642
-753.436170	-22.193057	5.985638
-751.521526	-30.536861	5.995635
-749.820198	-26.284774	6.005632
-747.473706	-25.959907	6.015629
-745.784243	-18.325473	6.025626
-744.017383	-28.854550	6.035622
-742.249327	-22.811585	6.045619
-740.422977	-26.775587	6.055616
-738.460091	-25.966260	6.065613
-736.392963	-22.817857	6.075610
-734.524903	-23.798067	6.085606
-732.838940	-30.172728	6.095603
-730.698523	-25.392388	6.105600
-728.904144	-25.925039	6.115597
-727.292136	-24.110707	6.125594
-725.230382	-29.670699	6.135590
-723.346814	-24.542999	6.145587
-721.159114	-28.771568	6.155584
-719.423212	-29.803276	6.165581
-717.785834	-23.429943	6.175578
-716.114669	-19.281953	6.185574
-713.834386	-22.911115	6.195571
-712.104724	-20.454009	6.205568
-710.176019	-22.249135	6.215565
-708.254549	-20.378452	6.225562
-706.493700	-24.685639	6.235558
-704.580948	-30.321277	6.245555
-702.699731	-26.061584	6.255552
-700.700945	-27.380016	6.265549
-698.961658	-23.329740	6.275546
-696.832056	-17.207142	6.285542
-695.381295	-22.521065	6.295539
-693.313424	-31.675608	6.305536
-691.380314	-28.703114	6.315533
-689.778669	-31.270154	6.325530
-687.721616	-20.225546	6.335526
-685.993475	-19.822340	6.345523
-683.758114	-18.205471	6.355520
-682.039190	-22.111216	6.365517
-680.101898	-21.544060	6.375514
-678.212024	-32.302744	6.385510
-676.360142	-29.509886	6.395507
-674.766520	-22.082711	6.405504
-672.634514	-28.781228	6.415501
-670.805192	-22.279058	6.425498
-668.952057	-21.221615	6.435494
-667.157837	-25.093591	6.445491
-664.995217	-22.910885	6.455488
-663.271151	-23.211205	6.465485
-661.657196	-23.091309	6.475482
-659.618164	-21.995668	6.485478
-657.345475	-27.279842	6.495475
-655.712755	-29.774458	6.505472
-654.195446	-21.384570	6.515469
-652.008882	-19.652508	6.525466
-650.192483	-24.945878	6.535462
-648.249820	-26.890023	6.545459
-646.421305	-27.203861	6.555456
-644.129061	-25.040267	6.565453
-642.697613	-33.237320	6.575450
-641.013863	-20.961474	6.585446
-638.700345	-30.074698	6.595443
-637.105416	-22.691913	6.605440
-635.302091	-22.546992	6.615437
-633.253475	-24.318583	6.625434
-631.658835	-24.962931	6.635430
-629.471755	-23.429874	6.645427
-627.486248	-27.378170	6.655424
-625.710949	-24.963027	6.665421
-624.043278	-22.263851	6.675418
-622.140818	-26.356766	6.685414
-619.913557	-27.915313	6.695411
-618.294556	-32.163461	6.705408
-616.337167	-28.752688	6.715405
-614.304196	-33.295909	6.725402
-612.739924	-29.200240	6.735398
-610.933219	-32.431552	6.745395
-609.205992	-27.847187	6.755392
-606.857775	-27.446669	6.765389
-604.817605	-26.752206	6.775386
-603.602624	-18.541345	6.785382
-601.396724	-26.429478	6.795379
-599.179435	-27.026434	6.805376
-597.686955	-31.428038	6.815373
-596.075915	-23.190447	6.825370
-593.889936	-23.965551	6.835366
-591.761226	-32.206071	6.845363
-590.052394	-29.972910	6.855360
-588.441259	-27.856769	6.865357
-586.231253	-24.427904	6.875354
-584.737351	-23.407745	6.885350
-582.642893	-27.281832	6.895347
-580.786778	-25.132190	6.905344
-578.970504	-21.360953	6.915341
-576.891943	-24.275677	6.925338
-574.921319	-24.037436	6.935334
-573.301929	-31.691332	6.945331
-571.220361	-20.652105	6.955328
-569.367225	-30.885385	6.965325
-567.660824	-19.617282	6.975322
-565.861496	-18.060121	6.985318
-563.826686	-30.303954	6.995315
-561.793439	-29.106254	7.005312
-560.111276	-23.832562	7.015309
-558.404854	-22.210031	7.025306
-556.760102	-22.653918	7.035302
-554.547667	-28.203106	7.045299
-552.187296	-25.101376	7.055296
-550.565947	-26.714653	7.065293
-548.710090	-28.371701	7.075290
-547.116502	-22.157029	7.085286
-545.328480	-22.633266	7.095283
-543.003317	-22.279526	7.105280
-541.365047	-28.531188	7.115277
-539.458489	-21.051264	7.125274
-537.548427	-24.963756	7.135270
-535.741576	-15.789516	7.145267
-534.011747	-24.637322	7.155264
-531.818492	-23.810934	7.165261
-530.396337	-20.938268	7.175258
-528.335119	-19.664481	7.185254
-526.226353	-20.547188	7.195251
-524.392184	-31.693179	7.205248
-522.545296	-24.088452	7.215245
-520.600581	-27.441213	7.225242
-518.836978	-14.865388	7.235238
-516.973339	-21.492498	7.245235
-515.148150	-23.735137	7.255232
-513.197989	-26.591406	7.265229
-511.553351	-18.635423	7.275226
-509.074172	-25.250311	7.285222
-507.299233	-23.483952	7.295219
-505.763899	-27.481831	7.305216
-503.823142	-28.129269	7.315213
-502.151532	-30.222635	7.325210
-500.058739	-20.959828	7.335206
-498.126172	-26.224276	7.345203
-496.232410	-25.343709	7.355200
-494.496512	-29.106776	7.365197
-492.500938	-30.443470	7.375194
-490.587335	-22.734109	7.385190
-488.896281	-22.165365	7.395187
-486.989632	-27.124093	7.405184
-485.000048	-22.886260	7.415181
-482.998326	-22.285023	7.425178
-481.606429	-20.547470	7.435174
-479.247529	-25.442630	7.445171
-477.548987	-16.383672	7.455168
-475.750976	-24.402348	7.465165
-473.709237	-24.156434	7.475162
-472.064024	-23.659304	7.485158
-469.982311	-22.606629	7.495155
-468.163391	-20.471482	7.505152
-466.384502	-27.511326	7.515149
-464.459493	-29.141460	7.525146
-462.164088	-26.840826	7.535142
-460.642081	-28.221868	7.545139
-458.555641	-29.146739	7.555136
-456.694497	-31.903485	7.565133
-454.853572	-23.596709	7.575130
-453.245862	-24.756174	7.585126
-451.496732	-26.850834	7.595123
-449.483498	-20.837309	7.605120
-447.615550	-25.121947	7.615117
-445.581919	-29.080942	7.625114
-443.776548	-23.057904	7.635110
-441.693985	-26.279462	7.645107
-440.134310	-29.196474	7.655104
-438.334286	-24.765703	7.665101
-436.056969	-15.197564	7.675098
-434.449255	-19.686951	7.685094
-432.616900	-18.757054	7.695091
-430.288126	-26.922027	7.705088
-428.571637	-24.456289	7.715085
-427.015401	-23.149147	7.725082
-425.169871	-18.725630	7.735078
-423.281057	-23.438311	7.745075
-421.050850	-29.148112	7.755072
-419.552824	-30.245831	7.765069
-417.665333	-30.379442	7.775066
-415.537893	-22.478373	7.785062
-413.618756	-21.420216	7.795059
-411.885871	-27.521119	7.805056
-409.797321	-21.865367	7.815053
-408.183024	-24.798976	7.825050
-406.171682	-23.477646	7.835046
-404.406655	-27.846869	7.845043
-402.335907	-23.242983	7.855040
-400.377003	-26.953173	7.865037
-398.872718	-28.587131	7.875034
-397.197276	-23.391187	7.885030
-395.084125	-25.217093	7.895027
-392.751729	-29.263220	7.905024
-391.167895	-31.096186	7.915021
-389.675762	-25.195194	7.925018
-387.491054	-31.000331	7.935014
-385.472570	-22.841842	7.945011
-383.404112	-22.895374	7.955008
-381.715386	-25.256650	7.965005
-380.216048	-23.971971	7.975002
-378.081049	-29.042863	7.984998
-376.461014	-29.031111	7.994995
-374.148377	-32.069875	8.004992
-372.226314	-28.381680	8.014989
-370.681992	-28.848878	8.024986
-369.058199	-30.710315	8.034982
-366.975556	-27.324062	8.044979
-364.909918	-25.109804	8.054976
-363.040091	-30.392554	8.064973
-360.950952	-28.114152	8.074970
-359.328265	-28.117022	8.084966
-357.450883	-30.003147	8.094963
-355.449836	-24.158116	8.104960
-353.740127	-31.996824	8.114957
-352.106528	-25.085780	8.124954
-349.828131	-20.980776	8.134950
-347.893231	-17.791965	8.144947
-346.057726	-23.457639	8.154944
-344.508452	-24.820857	8.164941
-342.570963	-26.661305	8.174938
-340.892381	-16.528545	8.184934
-338.331085	-19.910127	8.194931
-336.857825	-32.340461	8.204928
-334.922611	-28.106450	8.214925
-332.958000	-26.651284	8.224922
-331.196198	-18.489660	8.234918
-329.416901	-23.301629	8.244915
-327.303239	-24.225996	8.254912
-325.460852	-20.245571	8.264909
-323.863528	-20.411734	8.274906
-321.957181	-26.140803	8.284902
-319.916195	-23.527841	8.294899
-317.818117	-33.740056	8.304896
-316.298452	-29.000756	8.314893
-314.691937	-30.650982	8.324890
-312.532747	-24.108013	8.334886
-310.567027	-28.727098	8.344883
-308.421908	-27.760192	8.354880
-306.711137	-32.589624	8.364877
-305.126775	-29.951128	8.374874
-303.158044	-32.827564	8.384870
-301.298282	-23.969464	8.394867
-299.079398	-25.300595	8.404864
-297.384745	-30.070608	8.414861
-295.591311	-28.599140	8.424858
-293.690587	-25.180624	8.434854
-291.645682	-30.287589	8.444851
-290.073197	-27.784552	8.454848
-288.263642	-19.900510	8.464845
-286.000415	-31.616931	8.474842
-284.300276	-22.348080	8.484838
-282.438242	-20.203880	8.494835
-280.299086	-24.226955	8.504832
-278.463820	-23.175827	8.514829
-277.050022	-31.646190	8.524826
-275.077507	-23.652363	8.534822
-272.812798	-24.993943	8.544819
-271.171895	-23.918102	8.554816
-269.181901	-20.175924	8.564813
-267.422299	-19.643227	8.574810
-265.556364	-23.043218	8.584807
-263.796099	-23.440607	8.594803
-261.760611	-27.072915	8.604800
-259.910131	-26.576823	8.614797
-257.913358	-29.160863	8.624794
-256.175404	-25.062664	8.634791
-254.175626	-25.975107	8.644787
-252.300158	-27.571906	8.654784
-250.542094	-30.501517	8.664781
-248.883727	-24.765905	8.674778
-246.717990	-22.798041	8.684775
-244.754696	-24.693056	8.694771
-242.969829	-23.875432	8.704768
-240.953471	-28.726752	8.714765
-239.265225	-26.328997	8.724762
-237.218763	-22.676330	8.734759
-235.304951	-34.109577	8.744755
-233.502480	-33.981585	8.754752
-231.916896	-41.666194	8.764749
-229.839253	-33.507534	8.774746
-227.927775	-38.784200	8.784743
-226.001420	-35.860765	8.794739
-224.305319	-35.245272	8.804736
-222.518838	-30.308495	8.814733
-220.457137	-30.926061	8.824730
-218.530226	-31.132122	8.834727
-216.630957	-32.397960	8.844723
-214.851908	-35.690889	8.854720
-213.149004	-39.022188	8.864717
-210.649039	-43.920659	8.874714
-209.276768	-38.717249	8.884711
-207.689309	-41.426975	8.894707
-205.793291	-36.300829	8.904704
-203.412236	-40.142969	8.914701
-201.788308	-32.903436	8.924698
-199.915949	-33.560242	8.934695
-197.865430	-32.661822	8.944691
-196.014722	-42.191844	8.954688
-193.965000	-42.450641	8.964685
-192.399530	-48.412574	8.974682
-190.414463	-42.751164	8.984679
-188.675501	-48.641309	8.994675
-186.669605	-42.512703	9.004672
-184.908139	-43.115485	9.014669
-183.088781	-35.580290	9.024666
-181.238687	-41.406063	9.034663
-179.349622	-39.902401	9.044659
-177.259421	-34.756691	9.054656
-175.247155	-38.014177	9.064653
-173.674378	-35.053223	9.074650
-171.802154	-33.665286	9.084647
-169.869215	-39.460061	9.094643
-167.716686	-36.376883	9.104640
-166.056982	-35.982905	9.114637
-164.338881	-36.804539	9.124634
-162.558332	-41.292910	9.134631
-160.618350	-36.663205	9.144627
-158.257423	-40.707350	9.154624
-156.596806	-46.430240	9.164621
-155.135470	-38.923157	9.174618
-153.333877	-41.930696	9.184615
-151.046576	-41.122123	9.194611
-149.104530	-40.590031	9.204608
-147.375926	-44.700635	9.214605
-145.187644	-39.932120	9.224602
-143.440133	-36.975343	9.234599
-141.629302	-35.302855	9.244595
-139.716096	-37.559261	9.254592
-137.946122	-31.661379	9.264589
-135.992428	-28.821176	9.274586
-134.070262	-32.237935	9.284583
-132.400178	-33.405562	9.294579
-130.523909	-33.565579	9.304576
-128.395053	-36.644265	9.314573
-126.782104	-32.246556	9.324570
-124.884334	-30.448981	9.334567
-122.798676	-28.160338	9.344563
-121.131298	-34.841114	9.354560
-119.359028	-34.498222	9.364557
-117.419532	-26.933189	9.374554
-115.462636	-35.853273	9.384551
-113.449511	-25.453191	9.394547
-111.626190	-38.389258	9.404544
-109.736395	-29.092110	9.414541
-107.769707	-39.155308	9.424538
-106.093148	-31.188323	9.434535
-104.222762	-36.613078	9.444531
-102.359589	-38.443059	9.454528
-100.328904	-32.215696	9.464525
-98.776813	-34.652875	9.474522
-96.770579	-31.860494	9.484519
-94.725183	-34.269006	9.494515
-92.873996	-30.027700	9.504512
-91.223947	-33.235226	9.514509
-89.228369	-33.790028	9.524506
-87.261400	-27.833534	9.534503
-84.950440	-29.157057	9.544499
-83.631775	-29.243869	9.554496
-81.569626	-34.596571	9.564493
-79.760620	-32.551119	9.574490
-78.064290	-33.094487	9.584487
-75.974876	-32.907946	9.594483
-73.980022	-30.784771	9.604480
-72.695033	-28.859396	9.614477
-70.619888	-31.512631	9.624474
-68.217027	-31.470822	9.634471
-66.936043	-28.308510	9.644467
-64.867286	-32.211226	9.654464
-62.669980	-32.875555	9.664461
-60.912087	-30.454046	9.674458
-59.251913	-28.719566	9.684455
-57.434237	-27.048104	9.694451
-55.169536	-30.034718	9.704448
-53.566567	-30.053185	9.714445
-51.838776	-31.024704	9.724442
-49.687944	-28.575870	9.734439
-47.774278	-24.576594	9.744435
-46.217570	-35.526441	9.754432
-44.203350	-28.857459	9.764429
-42.206396	-29.185078	9.774426
-40.004128	-30.644376	9.784423
-38.524207	-28.413767	9.794419
-36.901626	-29.553227	9.804416
-34.871879	-38.813289	9.814413
-32.768326	-29.491751	9.824410
-30.811565	-27.690879	9.834407
-29.164168	-30.618473	9.844403
-27.055101	-29.511356	9.854400
-25.353139	-37.557039	9.864397
-23.473228	-29.845054	9.874394
-21.598300	-30.530554	9.884391
-19.575528	-33.786435	9.894387
-18.260299	-35.052117	9.904384
-15.908799	-35.690474	9.914381
-14.181147	-35.701961	9.924378
-12.158358	-36.351039	9.934375
-10.660769	-30.894338	9.944371
-8.387902	-30.272797	9.954368
-6.486171	-26.959993	9.964365
-4.901904	-11.273055	9.974362
-3.837535	14.729846	9.984359
-2.479012	57.588327	9.994355
-0.944662	112.077760	10.004352
0.000000	152.821427	10.009357
0.757794	186.025906	10.014362
1.348752	215.240632	10.019367
1.824383	243.508730	10.024371
2.143236	261.141808	10.029376
3.043088	283.077160	10.034381
3.034739	292.743744	10.039386
2.979046	300.426212	10.044391
3.403847	303.742771	10.049395
3.803367	319.565344	10.054400
4.128543	334.999249	10.059405
4.232249	321.091631	10.064410
3.775761	315.583851	10.069415
4.132254	305.682359	10.074419
3.746085	316.492578	10.079424
3.965324	321.656986	10.084429
3.887926	311.853080	10.089434
4.165173	329.874498	10.094439
4.051623	317.099088	10.099443
3.808519	320.011252	10.104448
4.077751	324.374486	10.109453
4.213219	338.518753	10.114458
4.226176	347.847664	10.119463
4.358870	347.763625	10.124467
4.303571	359.763734	10.129472
4.503053	358.005366	10.134477
4.304505	347.466979	10.139482
4.242248	365.094739	10.144487
4.541860	352.917293	10.149491
4.509291	369.792852	10.154496
4.434206	361.398333	10.159501
4.330545	361.897616	10.164506
4.265619	365.139336	10.169511
4.677989	361.497254	10.174515
4.523481	370.234727	10.179520
4.919978	373.440700	10.184525
4.890592	363.379943	10.189530
4.511900	373.916200	10.194535
4.729301	367.124513	10.199539
4.896943	370.606683	10.204544
5.103120	368.535010	10.209549
5.040400	375.807056	10.214554
4.920324	377.833864	10.219559
5.359993	395.491991	10.224563
5.479735	402.747564	10.229568
5.186573	400.411755	10.234573
5.163570	374.534754	10.239578
5.032395	397.063658	10.244583
5.586389	414.741421	10.249587
5.215757	415.519829	10.254592
5.457966	417.829481	10.259597
5.736894	416.108896	10.264602
5.861927	425.177130	10.269607
5.928137	404.194900	10.274611
5.393383	399.314581	10.279616
5.639621	405.348343	10.284621
5.742093	414.199395	10.289626
5.623637	422.371331	10.294631
5.747809	419.230942	10.299635
5.751018	434.728922	10.304640
5.908378	420.618687	10.309645
6.117531	422.641876	10.314650
6.050749	437.294737	10.319655
6.418106	426.915190	10.324659
5.872529	435.972120	10.329664
6.016106	431.688496	10.334669
6.024093	430.118357	10.339674
5.884764	445.342616	10.344679
6.050719	440.325290	10.349683
5.764113	440.339667	10.354688
6.360949	434.884611	10.359693
6.374784	434.283365	10.364698
6.540406	432.229190	10.369703
6.644247	434.092559	10.374707
6.501773	439.336780	10.379712
6.328337	437.432878	10.384717
6.666088	442.423886	10.389722
6.509697	439.266740	10.394727
6.570666	445.883580	10.399731
6.406797	447.914230	10.404736
6.805401	461.452097	10.409741
7.007212	456.172003	10.414746
6.896593	459.838925	10.419751
6.785510	449.466287	10.424755
6.775272	468.137704	10.429760
6.715346	482.231275	10.434765
7.234979	475.806072	10.439770
7.101460	487.139094	10.444775
7.197037	481.866472	10.449779
7.197021	481.363628	10.454784
7.799668	479.399015	10.459789
7.333731	463.615652	10.464794
6.871163	462.390221	10.469799
7.431063	483.416582	10.474803
7.293163	490.330091	10.479808
7.608583	491.070042	10.484813
7.690893	494.841821	10.489818
7.251110	493.492904	10.494823
7.379084	494.422026	10.499827
7.309051	496.798839	10.504832
7.237724	496.222213	10.509837
7.701989	488.913276	10.514842
7.639767	496.655237	10.519847
7.629797	492.806094	10.524851
7.544842	496.904174	10.529856
7.480438	505.496468	10.534861
7.573477	496.696585	10.539866
7.774789	522.891126	10.544871
7.794111	516.432163	10.549875
7.966256	531.529562	10.554880
8.096835	523.598889	10.559885
8.026717	538.391158	10.564890
7.907841	534.909461	10.569895
8.238570	534.571483	10.574899
8.113621	542.749253	10.579904
8.513144	537.700948	10.584909
8.486754	545.214867	10.589914
8.322236	533.480308	10.594919
8.347403	540.282675	10.599923
8.427609	537.412626	10.604928
8.314542	547.245894	10.609933
8.414030	536.047971	10.614938
8.374407	540.266566	10.619943
8.283840	525.836224	10.624947
8.807416	550.304679	10.629952
8.754945	562.932138	10.634957
8.925196	563.698401	10.639962
9.144212	569.214598	10.644967
9.018581	539.106898	10.649971
8.611301	546.251058	10.654976
8.797081	556.662721	10.659981
9.130142	563.854389	10.664986
9.257278	577.113962	10.669991
9.359897	566.087406	10.674995
8.964402	557.832188	10.680000
9.107016	561.155968	10.685005
9.114163	567.002427	10.690010
9.033547	580.498568	10.695015
9.394187	564.334096	10.700019
9.335759	585.987513	10.705024
9.199981	577.395966	10.710029
9.374468	580.345656	10.715034
8.889174	581.596528	10.720039
9.191464	577.662865	10.725043
9.305701	583.437055	10.730048
9.290777	582.178063	10.735053
9.482975	586.552088	10.740058
9.513076	605.538950	10.745063
9.520740	613.058512	10.750067
9.673231	610.019221	10.755072
9.805323	624.372467	10.760077
10.092937	611.961749	10.765082
9.889994	625.269282	10.770087
9.953699	612.999934	10.775091
9.822790	613.002093	10.780096
9.920932	613.675780	10.785101
10.042837	618.888937	10.790106
9.925703	610.308589	10.795111
10.088994	624.079686	10.800115
10.021025	628.242903	10.805120
10.017356	625.903462	10.810125
10.230667	627.779359	10.815130
10.349039	651.861600	10.820135
10.597491	645.955823	10.825139
10.188796	650.323204	10.830144
10.547700	658.909575	10.835149
10.667840	658.198323	10.840154
10.649798	656.749008	10.845159
11.013060	657.506570	10.850163
10.697840	649.254265	10.855168
10.535371	639.326509	10.860173
10.948698	647.778035	10.865178
10.490201	652.650107	10.870183
10.761929	637.280339	10.875187
10.927706	660.803094	10.880192
11.021635	661.717156	10.885197
10.920872	665.190166	10.890202
10.790480	674.237794	10.895207
11.072229	658.429582	10.900211
11.143076	672.199699	10.905216
11.330608	667.675602	10.910221
11.205524	668.681368	10.915226
11.047373	676.784083	10.920231
11.152822	668.843147	10.925235
11.037204	673.936509	10.930240
11.186924	671.411744	10.935245
11.401136	673.153460	10.940250
11.319933	677.708315	10.945255
11.444238	670.686904	10.950259
11.100866	684.199819	10.955264
11.106879	686.849967	10.960269
11.255845	686.697099	10.965274
11.467668	692.058369	10.970279
11.451521	704.938782	10.975283
11.685588	701.172089	10.980288
11.705539	693.762026	10.985293
11.474096	697.415163	10.990298
11.568727	708.324030	10.995303
11.712308	705.271949	11.000307
12.057396	716.369538	11.005312
11.954883	733.551572	11.010317
12.223790	729.831355	11.015322
12.463884	731.679339	11.020327
12.309080	718.735109	11.025331
11.955258	719.818362	11.030336
12.289231	725.641143	11.035341
12.384444	731.982988	11.040346
12.325292	742.443313	11.045351
12.448786	734.195105	11.050355
12.471226	734.071878	11.055360
12.399055	732.312638	11.060365
12.687269	731.287564	11.065370
12.508650	731.081285	11.070375
12.472225	739.054231	11.075379
11.964288	740.190452	11.080384
12.468338	725.460065	11.085389
12.800930	737.062721	11.090394
12.597733	734.775587	11.095399
12.943204	730.551139	11.100403
12.687100	743.305852	11.105408
12.974763	732.058841	11.110413
13.090080	734.972268	11.115418
12.716854	743.334833	11.120423
13.015774	733.462735	11.125427
12.754115	747.262302	11.130432
12.785140	736.589242	11.135437
13.028335	759.543133	11.140442
13.070082	776.858331	11.145447
13.399909	760.706441	11.150451
13.089785	774.212559	11.155456
12.896682	766.461116	11.160461
13.792214	766.794737	11.165466
13.432892	762.688999	11.170471
13.631195	768.881951	11.175475
13.813627	770.862142	11.180480
13.919021	766.694899	11.185485
13.878206	766.572299	11.190490
13.594227	771.181603	11.195495
13.935803	763.032640	11.200499
13.857681	758.002094	11.205504
13.605098	760.504262	11.210509
13.669155	758.761138	11.215514
13.705448	784.340637	11.220519
13.715803	771.809998	11.225523
14.006453	775.700011	11.230528
14.047151	778.631657	11.235533
14.074497	771.076869	11.240538
14.064292	777.411893	11.245543
14.257271	776.927144	11.250547
14.023785	768.923514	11.255552
14.041039	780.346260	11.260557
14.452661	772.966730	11.265562
14.060727	772.808666	11.270567
14.398695	770.127700	11.275571
14.145093	781.544760	11.280576
14.116941	765.923058	11.285581
14.133067	769.222905	11.290586
14.102383	780.784187	11.295591
14.454660	798.199697	11.300595
14.683935	799.243572	11.305600
14.689484	803.825633	11.310605
14.877699	805.647207	11.315610
14.736100	800.951631	11.320615
15.033389	800.929650	11.325619
14.721679	805.775206	11.330624
14.751822	813.641379	11.335629
15.097391	801.904095	11.340634
15.061282	816.768496	11.345639
15.300805	807.202296	11.350643
15.320755	803.480767	11.355648
15.146694	804.962720	11.360653
15.130536	798.200199	11.365658
15.281083	807.945865	11.370663
15.356169	800.552186	11.375667
15.278644	803.215680	11.380672
15.352405	806.430647	11.385677
15.287677	805.679487	11.390682
15.243700	809.118242	11.395687
15.519850	803.036092	11.400691
15.179327	814.675205	11.405696
15.082132	809.051579	11.410701
15.758796	810.495620	11.415706
15.442435	807.639881	11.420711
15.598435	806.665853	11.425715
15.700526	801.362114	11.430720
15.318841	813.930333	11.435725
15.416368	799.565914	11.440730
15.228763	816.655960	11.445735
15.484011	816.440406	11.450739
15.913448	820.166366	11.455744
15.686078	821.322501	11.460749
15.757777	830.120367	11.465754
15.556798	828.152994	11.470759
15.815493	814.112949	11.475763
15.811080	837.475473	11.480768
16.240379	846.328281	11.485773
16.593444	842.898974	11.490778
16.188551	853.763039	11.495783
16.701130	848.251883	11.500787
16.428258	839.708855	11.505792
16.670996	830.189438	11.510797
16.655052	813.272600	11.515802
16.247867	817.780141	11.520807
16.591163	820.551566	11.525811
16.211354	814.299636	11.530816
16.568804	842.316513	11.535821
16.909352	856.625702	11.540826
16.744530	856.395143	11.545831
17.013235	846.852649	11.550835
16.941933	843.771732	11.555840
16.838605	831.465760	11.560845
16.946492	846.870212	11.565850
16.825257	850.636700	11.570855
17.026040	850.622226	11.575859
16.872872	856.078043	11.580864
16.786758	853.324348	11.585869
17.418301	861.708080	11.590874
17.102623	863.956181	11.595879
17.293867	856.278223	11.600883
17.119722	859.113260	11.605888
17.001891	866.322587	11.610893
17.129615	860.272760	11.615898
17.134488	873.251687	11.620903
17.349454	850.520636	11.625907
17.248721	852.711586	11.630912
16.965057	859.290540	11.635917
17.619787	863.263650	11.640922
17.721949	871.370688	11.645927
17.879079	853.942848	11.650931
17.978002	858.357065	11.655936
17.349368	850.651386	11.660941
17.669937	865.743597	11.665946
17.799032	878.506379	11.670951
17.954002	872.954477	11.675955
18.218475	882.114302	11.680960
17.845078	890.715105	11.685965
17.848883	861.077327	11.690970
18.427196	884.997499	11.695975
18.082504	862.391173	11.700979
18.015095	873.072112	11.705984
18.289646	879.251374	11.710989
18.355767	860.868185	11.715994
18.196899	878.645234	11.720999
18.291110	864.394825	11.726003
18.529017	873.259252	11.731008
18.259271	879.634138	11.736013
18.499787	869.801226	11.741018
18.172146	885.256260	11.746023
18.495340	889.002338	11.751027
18.752006	898.934573	11.756032
18.918865	888.886308	11.761037
18.926911	889.684768	11.766042
18.145220	890.243321	11.771047
18.391255	883.106196	11.776051
18.646224	890.695271	11.781056
18.417619	896.172596	11.786061
18.489611	894.697858	11.791066
18.424268	899.791166	11.796071
18.694543	892.790523	11.801075
19.057067	903.300408	11.806080
19.005959	922.458338	11.811085
19.202578	912.783791	11.816090
19.370570	916.993038	11.821095
19.212628	917.392182	11.826099
19.226708	906.590808	11.831104
19.332872	912.322262	11.836109
19.450378	913.156884	11.841114
19.565703	914.837128	11.846119
19.112365	886.044155	11.851123
19.500980	906.175907	11.856128
19.618472	913.175043	11.861133
19.368589	905.426273	11.866138
19.608597	923.397600	11.871143
19.890243	915.146143	11.876147
20.057055	905.170416	11.881152
19.564580	902.495716	11.886157
19.791910	891.756539	11.891162
19.468866	892.868011	11.896167
19.897395	901.676820	11.901171
19.836678	909.589077	11.906176
19.818769	915.307204	11.911181
19.901251	905.313387	11.916186
19.856042	909.387896	11.921191
20.083924	917.473332	11.926195
20.212086	918.135937	11.931200
20.082328	921.295078	11.936205
20.455506	909.524919	11.941210
19.891060	916.364730	11.946215
20.113082	916.126089	11.951219
20.240336	926.766558	11.956224
19.920708	922.701752	11.961229
20.352421	916.856527	11.966234
20.152643	920.432126	11.971239
20.174126	918.074433	11.976243
20.490482	919.900817	11.981248
20.376773	928.233134	11.986253
20.972400	935.767902	11.991258
21.097117	925.677445	11.996263
21.148776	919.378731	12.001267
21.027873	910.347782	12.006272
20.781252	908.710963	12.011277
20.681898	905.123557	12.016282
20.885088	906.386074	12.021287
20.728319	903.776106	12.026291
20.477800	904.360331	12.031296
20.477076	902.472976	12.036301
20.928632	902.200880	12.041306
20.660308	906.413478	12.046311
21.050852	902.740053	12.051315
21.166818	907.138950	12.056320
21.013466	911.639152	12.061325
21.220114	907.662307	12.066330
21.019200	904.354458	12.071335
21.257396	899.271835	12.076339
21.143619	906.478170	12.081344
20.895983	905.150607	12.086349
21.273186	898.344225	12.091354
21.099545	880.747539	12.096359
21.039692	873.832675	12.101363
20.734448	877.461355	12.106368
20.313906	875.156822	12.111373
20.885914	870.552417	12.116378
20.466997	875.613797	12.121383
20.841947	870.990357	12.126387
20.710504	877.931406	12.131392
20.649115	872.115958	12.136397
20.815090	867.096905	12.141402
20.619146	875.920140	12.146407
20.715635	877.880937	12.151411
20.606318	885.701581	12.156416
20.710066	914.755728	12.161421
21.041413	911.072818	12.166426
20.958259	913.659956	12.171431
20.672926	901.865516	12.176435
20.789151	888.668165	12.181440
20.894761	881.723753	12.186445
20.775588	886.046602	12.191450
20.646403	892.023749	12.196455
20.789979	890.222193	12.201459
20.825209	889.153878	12.206464
20.919595	900.444564	12.211469
21.145782	887.753241	12.216474
20.880581	894.606818	12.221479
20.687344	885.812933	12.226483
21.069150	889.234263	12.231488
21.021617	890.686582	12.236493
20.947592	875.754919	12.241498
20.753832	893.557264	12.246503
21.064502	886.797771	12.251507
20.967133	881.431195	12.256512
20.933068	885.824052	12.261517
20.894713	878.285995	12.266522
20.990807	878.387570	12.271527
20.922100	889.803611	12.276531
20.915219	889.872723	12.281536
20.720950	882.641815	12.286541
20.900184	885.795822	12.291546
20.911712	898.522179	12.296551
20.818186	883.645659	12.301555
20.886177	872.261683	12.306560
20.786378	877.948700	12.311565
21.057125	876.383915	12.316570
20.675776	863.844705	12.321575
20.745182	857.687482	12.326579
20.516121	860.165414	12.331584
20.654280	878.860214	12.336589
21.127935	869.680845	12.341594
21.125772	869.973139	12.346599
20.331897	870.541519	12.351603
20.726880	872.427899	12.356608
20.854206	882.961089	12.361613
20.942441	881.453798	12.366618
20.772685	878.860099	12.371623
20.393882	869.837192	12.376627
20.792620	883.236660	12.381632
20.800062	881.264424	12.386637
21.121415	887.809975	12.391642
20.671761	881.689006	12.396647
20.965294	877.546920	12.401651
21.069088	869.667641	12.406656
20.620562	860.609338	12.411661
20.806827	856.796612	12.416666
20.852788	876.332462	12.421671
20.928433	859.494793	12.426675
20.889934	866.920133	12.431680
20.572032	870.068269	12.436685
20.861292	861.341739	12.441690
20.678793	865.768514	12.446695
20.805134	858.132446	12.451699
20.642082	856.441303	12.456704
20.459437	875.835412	12.461709
20.847155	881.356363	12.466714
21.125388	879.508100	12.471719
20.785029	871.215520	12.476723
20.775014	874.804998	12.481728
20.757441	876.328233	12.486733
20.982195	859.663908	12.491738
21.079716	862.517909	12.496743
21.063568	876.626958	12.501747
21.284295	868.522443	12.506752
21.025555	870.502047	12.511757
21.224874	869.027505	12.516762
20.872294	870.651481	12.521767
20.939255	879.259316	12.526771
20.936096	870.001449	12.531776
21.057931	881.481714	12.536781
20.820996	855.339132	12.541786
20.323120	862.074470	12.546791
20.785391	857.852647	12.551795
20.965776	851.889832	12.556800
20.689319	870.884146	12.561805
20.857022	866.934025	12.566810
20.932714	869.685060	12.571815
20.841992	857.932947	12.576819
20.985393	853.939395	12.581824
20.421489	855.041970	12.586829
20.713814	849.042380	12.591834
20.758042	860.145487	12.596839
20.638227	869.127680	12.601843
21.035548	868.701804	12.606848
20.775343	867.986547	12.611853
20.903881	859.479624	12.616858
20.661145	866.704142	12.621863
20.872179	872.054567	12.626867
21.010831	865.426601	12.631872
20.626679	858.363977	12.636877
20.959320	844.118139	12.641882
20.797886	851.033995	12.646887
20.427798	854.611509	12.651891
20.780231	860.756263	12.656896
20.964823	875.452268	12.661901
20.839830	865.247134	12.666906
20.679075	862.532150	12.671911
20.891117	861.441156	12.676915
20.743580	849.758825	12.681920
20.618370	857.085235	12.686925
20.842631	852.225630	12.691930
20.488530	865.985647	12.696935
20.796821	881.260400	12.701939
21.386364	874.667752	12.706944
20.997466	863.733556	12.711949
21.047937	860.463685	12.716954
20.744817	857.187919	12.721959
20.729587	842.874559	12.726963
20.707567	838.847468	12.731968
20.564464	847.480903	12.736973
20.959552	843.064001	12.741978
20.946840	845.824402	12.746983
20.759976	847.034003	12.751987
20.921396	840.315682	12.756992
20.865163	847.577467	12.761997
21.003007	842.173391	12.767002
20.796446	852.338753	12.772007
20.938268	855.651690	12.777011
21.306502	848.917726	12.782016
20.833981	857.783485	12.787021
21.006222	848.185411	12.792026
21.049176	855.074979	12.797031
20.912940	852.073804	12.802035
21.027856	854.377021	12.807040
20.825798	844.201540	12.812045
20.929673	828.828379	12.817050
20.843287	835.082535	12.822055
20.950310	834.598878	12.827059
20.875678	826.730734	12.832064
20.775880	839.790194	12.837069
20.803057	831.262394	12.842074
20.567072	818.427218	12.847079
20.493271	828.960907	12.852083
20.603514	838.342428	12.857088
21.042445	855.969699	12.862093
20.695291	834.628562	12.867098
20.424362	840.333396	12.872103
20.862019	851.287013	12.877107
20.726059	852.783395	12.882112
20.845035	848.934092	12.887117
20.955714	850.283901	12.892122
20.774611	847.680978	12.897127
20.927485	855.138081	12.902131
20.859768	839.251366	12.907136
20.748083	838.372070	12.912141
20.861748	833.968516	12.917146
20.601904	848.682548	12.922151
20.776888	844.758080	12.927155
20.856342	844.266204	12.932160
20.713662	848.572291	12.937165
20.786790	846.606930	12.942170
20.872298	854.145741	12.947175
20.603540	845.501124	12.952179
20.581182	841.986611	12.957184
20.409678	851.873561	12.962189
21.128515	849.668015	12.967194
20.793345	854.403785	12.972199
21.080388	855.179823	12.977203
20.982895	864.746674	12.982208
20.602159	854.966336	12.987213
20.807008	854.943329	12.992218
20.736766	858.854655	12.997223
20.720845	868.935216	13.002227
20.949267	861.456335	13.007232
20.795629	859.017769	13.012237
21.023063	857.951918	13.017242
20.873043	859.862140	13.022247
20.459479	853.128283	13.027251
20.848749	841.552736	13.032256
20.482043	849.835471	13.037261
20.947901	863.526211	13.042266
20.797332	863.810634	13.047271
21.092712	863.014652	13.052275
20.868357	846.073455	13.057280
20.429020	853.814250	13.062285
20.893290	852.707471	13.067290
20.835361	844.108080	13.072295
20.823708	852.635395	13.077299
20.871148	845.354915	13.082304
20.703159	847.458818	13.087309
20.756846	845.458710	13.092314
20.832838	850.212482	13.097319
20.954034	841.770608	13.102323
21.000089	848.877304	13.107328
20.814648	843.015419	13.112333
20.964355	841.755379	13.117338
20.955317	845.092374	13.122343
20.954597	853.029725	13.127347
21.240237	841.186847	13.132352
21.017759	848.435723	13.137357
21.332441	844.198807	13.142362
20.956524	861.520795	13.147367
21.071506	840.375609	13.152371
20.802055	831.552910	13.157376
20.476286	834.333276	13.162381
20.507963	842.334842	13.167386
20.709346	842.648288	13.172391
20.673929	855.233857	13.177395
20.704188	854.325614	13.182400
20.590321	860.439080	13.187405
20.499861	863.037625	13.192410
20.530091	844.969272	13.197415
20.422694	852.340148	13.202419
20.712642	852.399766	13.207424
20.653717	850.223647	13.212429
20.679661	854.624270	13.217434
20.878480	844.077338	13.222439
20.768101	857.193696	13.227443
21.047441	851.208791	13.232448
20.636950	848.420097	13.237453
20.684529	847.072264	13.242458
20.696868	848.740540	13.247463
20.594645	850.728295	13.252467
20.975020	842.800188	13.257472
20.809010	854.192296	13.262477
20.856467	851.800507	13.267482
20.590796	855.683076	13.272487
20.591208	855.760486	13.277491
21.054231	850.400741	13.282496
20.654446	851.049773	13.287501
21.001586	866.445262	13.292506
20.731180	856.611055	13.297511
20.771296	856.742059	13.302515
20.995134	863.581492	13.307520
20.845365	866.340100	13.312525
21.041863	850.708497	13.317530
20.904868	857.459604	13.322535
20.737647	864.542763	13.327539
20.976486	852.340688	13.332544
21.189137	862.613454	13.337549
21.122791	863.079992	13.342554
21.051946	860.532813	13.347559
20.911752	864.758869	13.352563
21.115549	866.328800	13.357568
20.852323	862.819582	13.362573
20.833508	837.963769	13.367578
20.820770	830.932598	13.372583
20.633136	824.708361	13.377587
20.546679	838.443800	13.382592
20.822319	844.208123	13.387597
20.958179	850.411070	13.392602
20.607783	845.042285	13.397607
20.830087	848.061677	13.402611
20.745496	849.139846	13.407616
20.381327	860.951506	13.412621
20.679011	850.518114	13.417626
20.502109	858.754812	13.422631
20.428814	864.834212	13.427635
20.882863	864.468676	13.432640
20.678756	859.857957	13.437645
20.899886	867.114151	13.442650
20.873839	859.358880	13.447655
20.642611	868.806710	13.452659
20.980736	859.768027	13.457664
20.777772	874.314525	13.462669
20.884734	857.948118	13.467674
21.092981	865.064436	13.472679
20.782084	856.370550	13.477683
21.241670	857.447085	13.482688
21.047148	869.032204	13.487693
21.028904	849.454502	13.492698
20.381282	842.237571	13.497703
20.565817	842.272999	13.502707
20.942920	860.190842	13.507712
20.686068	862.997280	13.512717
20.934540	868.147762	13.517722
21.158639	873.363636	13.522727
20.560420	851.503470	13.527731
20.919840	840.918309	13.532736
20.477946	841.474706	13.537741
20.477973	835.991685	13.542746
20.509405	861.567366	13.547751
20.825867	857.088881	13.552755
20.862626	862.305456	13.557760
21.184927	879.700615	13.562765
20.956783	868.501072	13.567770
21.038293	859.979571	13.572775
20.845249	844.749946	13.577779
20.747173	831.853338	13.582784
20.697698	838.705599	13.587789
20.807953	839.468831	13.592794
20.930582	844.830192	13.597799
20.849799	840.137519	13.602803
20.971462	833.446043	13.607808
20.636902	848.318652	13.612813
20.918359	836.667261	13.617818
20.732759	843.336226	13.622823
20.807986	846.792250	13.627827
20.747338	842.310835	13.632832
20.678663	843.850103	13.637837
20.928309	837.390533	13.642842
21.095893	838.534139	13.647847
20.791632	832.074604	13.652851
21.154198	835.155204	13.657856
20.815078	836.046880	13.662861
20.633987	842.027554	13.667866
20.964599	839.456562	13.672871
20.721936	841.654377	13.677875
21.190483	836.525574	13.682880
20.778932	841.486417	13.687885
20.782706	843.843630	13.692890
20.961789	842.309238	13.697895
20.958935	844.878826	13.702899
20.988659	843.551187	13.707904
21.026741	841.848467	13.712909
21.055783	841.555447	13.717914
20.894835	831.761360	13.722919
20.938824	813.735796	13.727923
20.739454	813.006109	13.732928
20.502675	814.890737	13.737933
20.643943	816.585756	13.742938
21.126036	830.254164	13.747943
20.324696	826.162133	13.752947
20.652408	823.069621	13.757952
20.912212	839.310876	13.762957
20.864409	843.630215	13.767962
20.831060	849.396511	13.772967
20.712197	845.878465	13.777971
20.730861	837.962317	13.782976
21.043069	848.530652	13.787981
20.951788	830.253821	13.792986
20.754211	821.892764	13.797991
20.319975	826.820949	13.802995
20.898233	821.346638	13.808000
20.793680	846.526077	13.813005
20.998587	845.184691	13.818010
21.041099	831.855641	13.823015
20.698139	829.964530	13.828019
20.479058	817.322207	13.833024
20.293715	846.949043	13.838029
20.478194	851.983565	13.843034
20.707439	849.400353	13.848039
20.813512	854.042092	13.853043
20.799725	853.516200	13.858048
20.487554	849.212099	13.863053
20.547520	852.443470	13.868058
20.932595	858.281810	13.873063
20.700223	848.573222	13.878067
20.802715	852.496421	13.883072
20.824760	850.517129	13.888077
21.231827	851.297679	13.893082
21.164186	846.352165	13.898087
20.709972	852.057850	13.903091
20.860470	845.912142	13.908096
20.646495	856.253736	13.913101
20.746149	857.103818	13.918106
20.851011	850.063343	13.923111
20.884861	846.170847	13.928115
20.645934	858.683218	13.933120
20.811853	861.120231	13.938125
20.961021	849.617667	13.943130
21.141834	856.521519	13.948135
20.894036	854.211515	13.953139
21.043924	840.389078	13.958144
20.486994	838.298697	13.963149
20.590397	842.070356	13.968154
20.825169	849.545934	13.973159
20.566680	862.207300	13.978163
20.755421	847.267663	13.983168
20.714520	857.103823	13.988173
20.685503	852.620515	13.993178
21.026281	856.764338	13.998183
21.038172	857.882315	14.003187
20.990797	854.179395	14.008192
21.068052	850.214163	14.013210
20.781629	842.442363	14.018227
20.544565	832.196271	14.023245
20.589084	834.089527	14.028263
21.135289	848.006808	14.033280
20.979764	866.196548	14.038298
21.073779	847.024479	14.043315
21.024607	837.667033	14.048333
20.769776	829.828855	14.053351
20.703733	831.327625	14.058368
20.539501	839.423379	14.063386
20.993781	840.640968	14.068403
21.041420	852.514255	14.073421
20.740304	865.778634	14.078439
21.176428	847.931501	14.083456
21.111936	865.463373	14.088474
21.145985	858.708503	14.093491
20.977797	860.539735	14.098509
21.069667	854.423711	14.103527
21.082508	862.640669	14.108544
21.174226	860.431942	14.113562
20.832972	865.874019	14.118579
20.974727	851.584717	14.123597
20.821965	863.136056	14.128615
21.371020	858.029321	14.133632
21.174570	847.528211	14.138650
21.047733	856.569660	14.143667
21.132896	855.711593	14.148685
20.923995	866.527871	14.153703
21.021698	862.603644	14.158720
21.074734	885.910071	14.163738
21.160390	890.433087	14.168755
21.544575	907.159654	14.173773
21.356785	905.599525	14.178791
21.376339	898.744704	14.183808
21.287113	901.049398	14.188826
21.049265	898.119322	14.193843
21.286717	890.813698	14.198861
21.129687	903.930079	14.203879
21.274012	901.678350	14.208896
21.214930	893.855319	14.213914
21.147137	907.811599	14.218931
21.390128	909.272099	14.223949
21.312630	919.546801	14.228967
21.623067	922.997381	14.233984
21.290894	931.838825	14.239002
21.286125	928.744156	14.244019
21.648887	924.002156	14.249037
21.609565	926.685850	14.254055
21.702518	922.605066	14.259072
21.892047	922.952557	14.264090
21.868093	925.638518	14.269107
21.921547	922.573890	14.274125
21.804562	926.490605	14.279143
21.978075	920.463776	14.284160
21.923061	916.282327	14.289178
21.881291	931.254558	14.294195
22.191691	918.829020	14.299213
21.859402	915.588395	14.304231
21.772500	910.694754	14.309248
21.990107	908.945701	14.314266
21.510292	922.095490	14.319283
21.872035	920.123678	14.324301
21.636850	926.638938	14.329319
21.775467	926.909609	14.334336
21.806996	919.069753	14.339354
21.655370	928.900120	14.344371
22.095929	919.044527	14.349389
21.947533	920.303191	14.354407
22.229135	924.548007	14.359424
21.752989	928.459087	14.364442
21.984532	917.851912	14.369459
21.761486	924.358943	14.374477
21.861207	919.828780	14.379495
22.001060	928.033382	14.384512
22.216542	922.150865	14.389530
21.997920	921.954709	14.394547
22.066430	932.846337	14.399565
21.816721	938.080364	14.404583
22.155338	949.087796	14.409600
22.258208	950.817608	14.414618
22.367146	960.513632	14.419635
22.614042	951.159228	14.424653
22.438931	963.478683	14.429671
22.431723	954.273341	14.434688
22.803430	951.916127	14.439706
22.728178	939.176136	14.444723
22.379153	926.972165	14.449741
22.562341	924.671763	14.454759
22.209895	926.231952	14.459776
22.194076	917.817645	14.464794
22.130851	922.399021	14.469811
22.525572	924.392160	14.474829
22.405188	942.038429	14.479847
22.561860	946.820689	14.484864
22.868541	941.258665	14.489882
22.346764	948.120084	14.494899
22.690446	934.295558	14.499917
22.827648	939.162717	14.504935
22.408191	934.396038	14.509952
22.827638	932.018629	14.514970
22.467734	938.748836	14.519987
22.754003	944.504553	14.525005
22.755523	953.942432	14.530023
23.031321	946.146971	14.535040
22.735799	925.190242	14.540058
22.420991	931.004068	14.545075
22.875755	938.851719	14.550093
23.019203	948.963791	14.555111
22.733384	929.238730	14.560128
22.739536	925.530429	14.565146
22.557864	950.241317	14.570163
22.869344	944.761894	14.575181
22.574264	952.552972	14.580199
22.783960	956.662978	14.585216
23.209462	958.596158	14.590234
23.019767	950.113612	14.595251
22.932732	950.324320	14.600269
22.556145	959.043879	14.605287
22.815221	955.748252	14.610304
23.054567	946.802459	14.615322
23.038799	951.793118	14.620339
23.069082	955.647028	14.625357
22.893127	954.534880	14.630375
22.499291	945.266942	14.635392
22.981652	945.618065	14.640410
22.475797	961.447692	14.645427
22.951566	963.207692	14.650445
23.121919	969.324817	14.655463
23.261298	970.894656	14.660480
23.661494	978.079365	14.665498
23.485128	983.718552	14.670515
23.505082	961.549015	14.675533
23.502899	959.438617	14.680551
23.352173	951.967577	14.685568
23.395786	954.010427	14.690586
23.059259	948.606041	14.695603
22.940678	952.488412	14.700621
23.509266	952.116366	14.705639
23.453088	979.113286	14.710656
23.653319	975.506150	14.715674
23.542383	954.323315	14.720691
23.885353	933.002051	14.725709
23.689646	938.529477	14.730727
23.614584	956.141795	14.735744
24.103471	939.258241	14.740762
23.475397	941.703938	14.745779
23.497648	944.244111	14.750797
23.651033	935.625059	14.755815
24.025884	948.119475	14.760832
23.876899	939.235623	14.765850
23.503099	942.502762	14.770867
23.898200	939.023426	14.775885
23.472461	936.415884	14.780903
23.468955	944.890319	14.785920
23.851850	935.389969	14.790938
23.805154	944.343188	14.795955
23.696625	947.703297	14.800973
23.700349	948.899949	14.805991
23.739051	944.900169	14.811008
23.645274	949.195424	14.816026
23.571121	953.174527	14.821043
23.442927	940.980939	14.826061
23.731199	964.539405	14.831079
23.512714	976.389172	14.836096
23.519372	970.689375	14.841114
24.028786	982.761247	14.846131
24.169652	969.821596	14.851149
24.236830	975.381039	14.856167
24.064401	975.053249	14.861184
24.083079	962.172417	14.866202
24.131336	971.884419	14.871219
24.129641	967.809279	14.876237
24.557323	960.318342	14.881255
24.111677	964.580061	14.886272
24.504939	962.664564	14.891290
24.385706	951.600516	14.896307
24.079467	938.296485	14.901325
23.902335	956.126424	14.906343
24.080086	944.908052	14.911360
24.041721	951.042729	14.916378
23.917626	975.536843	14.921395
24.215135	971.620044	14.926413
24.427987	969.727027	14.931431
24.167634	977.599094	14.936448
24.531749	965.915265	14.941466
24.636225	976.245925	14.946483
24.496295	969.575379	14.951501
24.282188	977.241873	14.956519
24.267688	976.634070	14.961536
24.672597	970.553011	14.966554
24.374358	969.641258	14.971571
24.171247	979.031568	14.976589
24.543552	973.325361	14.981607
24.348312	978.143310	14.986624
24.652041	973.382396	14.991642
24.567628	983.101408	14.996659
24.600431	965.977540	15.001677
24.681640	964.984820	15.006695
24.499683	982.769944	15.011712
24.759797	971.779083	15.016730
24.659478	974.955422	15.021747
24.526854	973.148965	15.026765
24.613959	974.255244	15.031783
24.408340	973.962634	15.036800
24.774202	958.407406	15.041818
24.593090	977.362692	15.046835
24.789090	974.040942	15.051853
24.925314	986.521541	15.056871
24.826399	997.375429	15.061888
25.344159	995.583213	15.066906
24.998126	978.835922	15.071923
25.135389	970.131334	15.076941
24.968173	970.483816	15.081959
24.707178	971.972795	15.086976
24.993123	965.968913	15.091994
25.134522	968.158187	15.097011
25.067643	978.273938	15.102029
25.368595	963.015342	15.107047
24.852633	963.503668	15.112064
25.207734	958.125819	15.117082
25.166714	953.575622	15.122099
24.862150	963.471302	15.127117
25.027088	975.344858	15.132135
25.055459	988.223323	15.137152
25.445165	992.924389	15.142170
25.416678	995.123459	15.147187
25.129309	976.513830	15.152205
25.382675	975.748476	15.157223
25.260470	982.668876	15.162240
25.179095	976.751887	15.167258
25.375247	990.360204	15.172275
25.345446	1003.129986	15.177293
25.790306	991.678645	15.182311
25.193498	981.058824	15.187328
25.267064	983.067014	15.192346
25.568980	992.088928	15.197363
25.637370	992.134852	15.202381
25.582207	994.305143	15.207399
25.513800	998.155929	15.212416
25.532652	996.042172	15.217434
25.893742	992.623303	15.222451
25.169489	980.218015	15.227469
25.875851	986.833239	15.232487
25.948375	1000.226906	15.237504
25.948858	985.497545	15.242522
25.910591	974.323041	15.247539
25.791083	971.028018	15.252557
25.905323	961.663305	15.257575
25.303696	970.601230	15.262592
25.502749	954.073763	15.267610
25.588588	975.484374	15.272627
25.662283	985.878151	15.277645
25.851762	987.534380	15.282663
25.837386	989.190090	15.287680
26.056338	997.669974	15.292698
26.223181	989.498620	15.297715
25.899609	993.871436	15.302733
25.863307	991.977257	15.307751
25.892378	993.990972	15.312768
25.976274	988.930067	15.317786
25.846546	992.538953	15.322803
25.710356	996.134714	15.327821
26.328411	984.564522	15.332839
25.929314	996.734115	15.337856
26.064932	989.299183	15.342874
26.358337	992.832718	15.347891
25.838941	996.066462	15.352909
26.305438	989.830858	15.357927
26.337468	984.908785	15.362944
26.082146	985.152626	15.367962
26.240037	986.868948	15.372979
26.048174	998.824597	15.377997
26.421794	985.003114	15.383015
26.006468	987.443201	15.388032
26.372076	983.309476	15.393050
26.346799	986.774290	15.398067
26.487856	993.160361	15.403085
26.301387	981.007493	15.408103
26.358616	988.158821	15.413120
26.346366	986.594280	15.418138
26.511362	989.802237	15.423155
26.003055	986.039122	15.428173
26.230742	991.090064	15.433191
26.398127	1005.387233	15.438208
26.429248	1023.906044	15.443226
26.805873	1011.661770	15.448243
26.646584	1013.483737	15.453261
26.653401	1013.670040	15.458279
26.474486	1008.457566	15.463296
26.714794	1015.222638	15.468314
26.975402	1012.069897	15.473331
26.818273	1020.422589	15.478349
27.078487	1025.221395	15.483367
26.841252	1013.992080	15.488384
27.092555	1005.325910	15.493402
26.886344	1007.150641	15.498419
26.526570	990.380360	15.503437
26.370537	1010.555475	15.508455
26.627480	1015.405135	15.513472
26.680001	1016.208627	15.518490
26.921616	1016.091646	15.523507
26.673239	1007.037991	15.528525
26.950374	1018.064720	15.533543
27.100637	1020.309216	15.538560
26.831819	1015.260513	15.543578
26.879175	1015.308218	15.548595
26.462322	1028.639966	15.553613
26.781774	1022.125786	15.558631
26.870112	1044.654499	15.563648
27.260626	1046.912589	15.568666
27.916230	1039.748623	15.573683
27.460129	1043.901922	15.578701
27.463704	1044.098181	15.583719
27.809707	1026.776427	15.588736
27.407514	1014.212780	15.593754
27.398679	1005.021822	15.598771
27.429294	1016.953014	15.603789
27.310971	1003.279186	15.608807
27.226333	1010.885724	15.613824
27.225998	1010.878116	15.618842
27.267703	1003.554106	15.623859
27.173426	1019.635898	15.628877
27.635419	1037.390743	15.633895
27.593958	1033.507541	15.638912
27.737888	1033.091541	15.643930
27.857772	1023.757348	15.648947
27.586431	1020.077551	15.653965
27.259949	1005.565481	15.658983
27.457253	1023.560721	15.664000
27.577257	1033.656143	15.669018
27.941726	1027.578365	15.674035
28.007107	1030.959519	15.679053
27.469112	1029.271189	15.684071
27.707900	1026.085746	15.689088
28.057554	1031.423983	15.694106
27.693045	1018.144901	15.699123
27.550692	1034.751892	15.704141
27.883737	1028.484075	15.709159
28.094310	1039.858058	15.714176
28.040208	1039.193648	15.719194
28.238950	1026.820432	15.724211
27.760717	1026.508380	15.729229
27.818097	1022.401781	15.734247
27.521360	1031.460999	15.739264
27.777720	1040.874020	15.744282
27.980638	1038.107993	15.749299
28.030915	1037.408060	15.754317
28.183161	1032.971729	15.759335
28.169816	1047.774383	15.764352
28.073041	1039.448421	15.769370
28.419328	1032.728612	15.774387
28.326457	1031.971287	15.779405
28.520201	1034.525022	15.784423
28.531116	1027.278269	15.789440
28.422721	1032.879894	15.794458
28.500117	1029.089419	15.799475
28.160676	1035.435742	15.804493
28.404394	1030.910892	15.809511
28.579618	1037.011540	15.814528
28.445920	1033.149341	15.819546
28.677361	1020.261265	15.824563
28.332935	1015.775168	15.829581
28.363464	1018.030894	15.834599
28.601430	1019.770628	15.839616
28.417725	1016.908968	15.844634
28.718820	1036.990765	15.849651
28.696896	1031.696616	15.854669
28.669633	1017.330290	15.859687
28.646449	1017.622049	15.864704
28.448830	1021.133234	15.869722
28.896151	1019.451349	15.874739
28.716479	1028.864694	15.879757
28.619344	1032.114468	15.884775
28.930296	1028.681565	15.889792
28.631906	1030.436059	15.894810
28.857973	1035.496712	15.899827
28.686732	1030.909059	15.904845
28.686587	1031.838926	15.909863
28.780680	1026.038647	15.914880
28.623627	1033.047997	15.919898
29.208025	1034.496531	15.924915
28.778628	1033.728386	15.929933
28.523776	1040.608622	15.934951
28.877070	1033.080749	15.939968
28.593160	1034.958773	15.944986
28.930702	1026.782195	15.950003
28.759596	1040.376775	15.955021
29.209357	1050.932413	15.960039
29.454587	1055.151610	15.965056
28.998908	1041.498517	15.970074
29.295117	1029.760974	15.975091
28.875115	1041.723157	15.980109
29.027907	1048.719277	15.985127
29.479684	1053.770680	15.990144
29.118337	1062.660899	15.995162
29.204243	1054.557472	16.000179
29.340745	1059.269056	16.005197
29.498396	1049.096708	16.010215
29.682237	1051.950895	16.015232
29.517479	1055.924027	16.020250
30.082710	1053.325152	16.025267
29.730138	1039.112932	16.030285
29.264520	1036.838914	16.035303
29.299306	1026.517866	16.040320
29.260447	1034.625193	16.045338
29.446334	1036.829404	16.050355
29.496536	1054.629498	16.055373
29.379130	1057.950149	16.060391
29.801200	1060.211075	16.065408
29.921342	1056.618266	16.070426
29.604195	1057.372181	16.075443
29.666878	1051.359828	16.080461
29.710682	1055.565533	16.085479
30.012673	1049.779278	16.090496
30.117762	1056.735819	16.095514
30.124016	1052.873316	16.100531
29.886526	1050.603810	16.105549
30.205978	1058.809730	16.110567
30.158495	1049.340195	16.115584
30.018796	1041.085570	16.120602
29.983042	1034.683091	16.125619
29.832941	1034.834647	16.130637
30.079044	1043.860777	16.135655
30.140698	1046.762764	16.140672
30.110437	1045.518835	16.145690
30.261421	1051.579311	16.150707
30.395415	1044.158766	16.155725
29.799448	1037.136212	16.160743
30.289536	1031.947589	16.165760
30.345953	1045.235331	16.170778
30.437543	1049.357909	16.175795
30.283394	1040.932559	16.180813
29.778352	1055.491177	16.185831
30.169036	1056.278490	16.190848
30.273971	1058.566400	16.195866
30.304297	1055.003646	16.200883
30.196109	1063.966746	16.205901
30.366121	1058.357263	16.210919
30.426721	1050.599214	16.215936
30.004104	1066.517924	16.220954
30.231691	1053.344148	16.225971
30.259352	1057.495800	16.230989
30.274361	1075.915003	16.236007
30.666430	1088.089049	16.241024
30.643605	1085.385758	16.246042
30.848870	1083.972129	16.251059
31.020201	1088.621540	16.256077
30.702905	1076.113511	16.261095
30.793703	1058.146594	16.266112
30.545518	1067.176068	16.271130
30.809826	1076.814358	16.276147
30.989305	1081.375952	16.281165
30.774134	1088.186962	16.286183
31.135163	1076.302192	16.291200
30.841100	1073.944179	16.296218
30.849502	1070.504465	16.301235
30.705938	1077.909654	16.306253
30.751033	1092.418320	16.311271
31.297049	1074.814502	16.316288
30.902321	1085.245307	16.321306
31.115250	1082.026224	16.326323
31.392911	1083.690423	16.331341
31.230465	1076.804771	16.336359
31.223727	1080.368895	16.341376
30.723215	1077.026076	16.346394
31.112385	1076.435684	16.351411
31.353209	1073.852365	16.356429
31.370782	1082.257453	16.361447
31.544203	1071.483260	16.366464
31.083085	1084.446172	16.371482
31.268809	1075.869069	16.376499
31.706415	1070.534650	16.381517
31.079233	1077.703943	16.386535
31.327357	1076.318086	16.391552
31.132501	1087.893620	16.396570
31.402338	1076.897983	16.401587
31.475999	1084.896158	16.406605
31.148870	1083.608338	16.411623
31.692193	1063.958489	16.416640
31.570245	1080.287003	16.421658
31.250621	1078.659792	16.426675
31.128274	1093.140108	16.431693
31.548981	1099.926785	16.436711
31.520668	1099.409268	16.441728
31.379232	1104.814845	16.446746
31.888297	1100.301136	16.451763
32.111642	1094.785379	16.456781
31.904985	1105.853156	16.461799
32.028366	1101.032877	16.466816
32.346446	1108.874108	16.471834
32.040725	1093.532811	16.476851
32.325927	1097.258014	16.481869
32.242702	1100.266489	16.486887
32.092556	1094.354128	16.491904
32.244817	1104.611193	16.496922
32.083108	1080.670930	16.501939
32.302225	1086.464156	16.506957
31.652468	1083.708272	16.511975
32.093607	1092.634115	16.516992
32.395737	1100.128678	16.522010
32.165185	1093.467808	16.527027
32.567570	1096.150298	16.532045
32.377155	1102.221201	16.537063
32.223745	1081.642694	16.542080
31.954094	1086.419063	16.547098
31.997866	1100.481216	16.552115
32.484529	1088.238205	16.557133
32.511688	1106.633487	16.562151
32.478068	1099.447282	16.567168
32.586283	1100.444814	16.572186
32.550036	1102.141777	16.577203
32.388758	1093.483156	16.582221
32.168981	1103.593493	16.587239
31.918048	1100.847929	16.592256
32.244715	1099.356736	16.597274
32.367081	1100.976493	16.602291
32.521721	1108.854802	16.607309
32.628842	1131.122681	16.612327
32.842047	1120.134471	16.617344
32.978414	1127.507624	16.622362
32.435332	1124.915614	16.627379
33.043616	1129.422992	16.632397
32.913564	1129.835616	16.637415
33.119375	1117.794672	16.642432
33.221579	1129.126236	16.647450
33.064637	1117.574151	16.652467
33.238897	1111.661954	16.657485
32.861613	1101.782521	16.662503
33.009204	1097.054334	16.667520
33.106348	1098.892042	16.672538
32.996277	1111.931122	16.677555
33.262754	1106.032533	16.682573
33.147246	1115.051887	16.687591
33.397740	1119.886882	16.692608
32.770586	1111.066601	16.697626
33.008925	1117.157217	16.702643
33.137025	1112.540672	16.707661
33.010556	1128.363454	16.712679
33.364645	1118.422420	16.717696
33.510757	1118.386736	16.722714
33.267914	1125.442846	16.727731
33.436542	1124.387410	16.732749
32.978765	1117.569289	16.737767
33.467136	1119.903020	16.742784
33.667899	1128.993063	16.747802
33.396369	1118.228453	16.752819
33.642002	1115.718291	16.757837
33.600532	1121.652191	16.762855
33.593588	1127.980130	16.767872
33.809363	1116.777583	16.772890
33.365439	1126.966156	16.777907
33.569842	1118.285378	16.782925
33.648216	1135.079074	16.787943
33.807703	1139.293095	16.792960
34.232708	1153.063265	16.797978
33.828201	1139.074731	16.802995
34.151046	1122.543061	16.808013
33.933366	1122.115518	16.813031
33.645274	1122.959183	16.818048
34.126778	1113.638044	16.823066
33.955770	1125.848444	16.828083
34.151408	1116.964574	16.833101
33.954870	1117.600156	16.838119
34.001317	1131.287537	16.843136
33.921803	1134.800362	16.848154
33.895134	1152.628567	16.853171
34.294712	1143.636650	16.858189
34.253272	1147.072619	16.863207
34.175205	1152.070136	16.868224
34.398288	1150.634784	16.873242
34.139197	1145.534146	16.878259
34.408473	1142.751225	16.883277
34.152132	1140.840210	16.888295
34.226842	1136.219588	16.893312
34.356433	1144.056294	16.898330
34.341421	1141.770166	16.903347
34.480504	1132.774184	16.908365
34.458810	1150.419125	16.913383
34.434711	1144.741467	16.918400
34.881048	1137.225443	16.923418
34.450045	1146.218056	16.928435
34.324745	1141.879440	16.933453
34.276968	1153.691115	16.938471
34.423861	1165.956239	16.943488
34.715983	1167.784881	16.948506
34.841717	1181.465956	16.953523
35.197795	1166.066224	16.958541
35.097767	1173.694178	16.963559
35.205535	1175.371326	16.968576
35.095664	1166.042225	16.973594
34.813542	1154.159295	16.978611
35.124666	1162.744125	16.983629
34.796032	1156.369426	16.988647
35.297066	1157.913067	16.993664
35.178722	1166.324150	16.998682
35.020795	1162.390276	17.003699
35.329565	1173.316126	17.008717
35.141539	1172.084763	17.013735
35.326896	1160.394683	17.018752
35.367611	1159.477620	17.023770
35.084151	1147.170196	17.028787
35.130899	1146.919128	17.033805
35.121653	1176.347094	17.038823
35.322431	1167.032941	17.043840
35.643474	1161.816179	17.048858
35.192613	1173.926535	17.053875
35.406273	1169.609356	17.058893
35.480212	1169.836865	17.063911
35.102863	1166.175509	17.068928
35.733523	1164.989754	17.073946
35.140649	1165.504507	17.078963
35.516845	1171.105976	17.083981
35.432508	1165.990044	17.088999
35.439891	1165.320541	17.094016
35.688965	1166.183928	17.099034
35.450246	1174.340511	17.104051
35.475555	1180.831642	17.109069
35.682988	1188.402702	17.114087
35.851908	1199.166834	17.119104
36.283372	1192.128204	17.124122
36.159925	1198.463743	17.129139
35.913893	1199.313288	17.134157
36.228368	1191.793098	17.139175
36.200719	1187.816417	17.144192
36.263842	1165.205530	17.149210
35.874658	1167.215190	17.154227
36.279200	1150.711356	17.159245
35.896926	1158.186117	17.164263
35.735001	1166.437413	17.169280
36.207873	1178.785838	17.174298
36.496612	1188.196939	17.179315
36.353762	1193.285025	17.184333
36.387547	1185.708932	17.189351
36.099585	1188.798840	17.194368
36.282349	1181.040115	17.199386
36.253559	1183.693862	17.204403
36.495240	1183.502939	17.209421
36.550828	1179.665567	17.214439
36.426339	1187.578998	17.219456
36.637263	1175.153377	17.224474
36.758716	1183.065334	17.229491
37.052574	1173.690715	17.234509
36.681855	1179.589060	17.239527
36.733437	1183.046382	17.244544
37.061505	1184.353346	17.249562
36.395561	1179.120957	17.254579
36.588819	1186.105971	17.259597
36.634555	1180.033347	17.264615
36.642153	1179.038196	17.269632
36.850438	1177.965421	17.274650
36.757534	1187.055146	17.279667
36.505468	1174.980216	17.284685
36.847030	1184.033681	17.289703
36.557223	1187.466800	17.294720
36.770084	1189.267188	17.299738
36.616328	1213.330709	17.304755
37.029397	1215.780285	17.309773
37.412036	1203.048831	17.314791
37.418735	1214.447603	17.319808
37.717052	1211.801608	17.324826
37.472195	1210.867167	17.329843
37.250156	1215.810590	17.334861
37.257242	1204.557889	17.339879
37.213392	1209.192895	17.344896
37.691320	1197.953195	17.349914
37.412252	1197.370274	17.354931
37.359114	1206.271200	17.359949
37.640683	1203.259793	17.364967
37.698341	1206.091664	17.369984
37.863447	1198.121816	17.375002
37.564429	1173.830493	17.380019
37.563393	1178.562479	17.385037
37.720576	1188.726012	17.390055
37.692313	1194.259863	17.395072
37.947559	1194.357784	17.400090
37.784364	1182.465300	17.405107
37.470935	1178.782735	17.410125
38.009738	1174.599314	17.415143
37.924713	1195.040211	17.420160
37.779079	1195.765206	17.425178
37.905477	1193.734940	17.430195
37.903784	1195.783477	17.435213
37.991213	1190.283068	17.440231
37.836989	1194.216805	17.445248
38.122463	1191.418707	17.450266
38.196581	1198.731039	17.455283
37.806275	1212.238043	17.460301
38.047943	1197.361462	17.465319
38.059287	1199.271068	17.470336
38.342127	1206.594160	17.475354
38.072229	1205.597647	17.480371
38.016314	1197.867540	17.485389
38.059603	1197.955221	17.490407
38.309579	1208.490930	17.495424
38.606902	1223.289833	17.500442
38.406322	1226.362667	17.505459
38.239275	1230.111270	17.510477
39.164583	1225.027775	17.515495
38.644320	1216.017348	17.520512
38.561837	1206.863176	17.525530
38.740197	1208.233344	17.530547
38.615990	1202.233432	17.535565
39.025693	1215.921161	17.540583
38.328688	1209.929228	17.545600
38.725332	1218.885842	17.550618
39.091998	1230.362496	17.555635
38.880884	1234.684414	17.560653
38.967953	1228.504505	17.565671
38.961727	1219.034571	17.570688
38.937199	1222.585838	17.575706
38.775160	1227.326214	17.580723
39.002648	1216.776098	17.585741
38.978469	1225.927246	17.590759
38.690143	1225.883771	17.595776
39.230886	1219.994878	17.600794
38.913847	1225.453674	17.605811
38.949157	1222.921982	17.610829
39.288054	1231.118609	17.615847
39.022947	1227.764950	17.620864
38.989582	1228.770914	17.625882
38.975637	1237.124490	17.630899
39.425759	1245.960907	17.635917
39.604582	1256.437213	17.640935
39.666970	1266.814120	17.645952
39.639965	1243.473447	17.650970
39.874893	1231.459227	17.655987
39.293069	1237.266995	17.661005
39.716555	1220.267707	17.666023
39.402616	1240.641358	17.671040
39.453971	1246.895557	17.676058
39.680585	1257.285591	17.681075
39.554150	1260.788625	17.686093
40.013804	1251.507064	17.691111
39.651772	1265.070956	17.696128
39.877799	1256.735857	17.701146
39.811212	1250.464041	17.706163
39.594713	1260.492166	17.711181
39.873286	1249.768712	17.716199
39.775182	1255.702261	17.721216
39.911802	1250.444094	17.726234
40.243974	1254.125669	17.731251
40.108300	1247.109823	17.736269
40.119898	1247.408624	17.741287
39.780205	1251.640942	17.746304
40.114439	1255.874319	17.751322
40.309981	1263.085521	17.756339
40.119826	1273.649000	17.761357
40.298610	1260.894951	17.766375
40.280291	1262.394019	17.771392
40.400546	1273.351584	17.776410
40.567331	1254.263326	17.781427
40.358082	1265.562871	17.786445
40.863006	1257.567109	17.791463
40.719678	1258.469490	17.796480
40.934301	1262.514306	17.801498
41.073643	1255.586729	17.806515
40.614395	1259.537670	17.811533
40.886154	1245.656681	17.816551
40.884510	1261.116782	17.821568
40.574533	1248.516199	17.826586
40.920887	1246.645901	17.831603
40.766257	1267.124742	17.836621
40.960519	1244.406301	17.841639
40.777251	1262.920285	17.846656
40.752341	1259.695051	17.851674
41.035171	1263.364048	17.856691
40.732686	1272.507701	17.861709
40.713866	1264.958832	17.866727
40.911426	1267.887954	17.871744
40.765868	1255.007886	17.876762
40.831951	1273.271331	17.881779
41.228554	1284.752692	17.886797
41.474287	1291.919725	17.891815
41.409760	1296.010643	17.896832
41.288449	1290.521465	17.901850
41.523118	1285.033718	17.906867
41.457380	1292.182785	17.911885
41.385579	1295.035321	17.916903
41.181109	1295.415773	17.921920
41.353160	1289.187678	17.926938
41.691491	1283.541826	17.931955
41.458418	1295.386315	17.936973
41.668562	1286.605420	17.941991
41.417352	1298.962463	17.947008
41.181980	1287.323650	17.952026
41.743595	1302.535089	17.957043
41.627540	1293.985538	17.962061
41.556561	1298.044453	17.967079
41.838236	1307.143727	17.972096
41.877795	1316.563192	17.977114
41.939806	1311.576452	17.982131
42.113472	1322.516098	17.987149
41.980006	1321.960286	17.992167
42.447651	1314.067967	17.997184
42.109752	1322.927862	18.002202
42.316489	1309.503923	18.007219
42.212417	1318.346973	18.012237
42.019695	1313.182207	18.017255
42.294297	1307.257074	18.022272
42.417060	1322.999420	18.027290
42.983993	1304.419861	18.032307
42.412648	1318.846168	18.037325
42.408183	1303.030311	18.042343
42.513049	1316.469451	18.047360
42.259758	1318.493637	18.052378
42.652969	1299.572127	18.057395
42.859333	1311.230142	18.062413
42.723611	1311.638955	18.067431
42.557765	1308.656411	18.072448
42.488417	1300.437608	18.077466
42.930038	1311.137883	18.082483
42.528578	1319.460500	18.087501
42.585466	1309.978869	18.092519
42.481509	1308.841051	18.097536
42.517258	1308.096232	18.102554
42.837303	1316.676586	18.107571
42.920874	1330.509245	18.112589
43.102356	1335.739138	18.117607
43.264436	1337.267645	18.122624
43.585974	1335.006464	18.127642
43.593299	1311.134815	18.132659
42.953300	1316.800881	18.137677
42.906573	1303.727257	18.142695
43.212882	1318.409994	18.147712
43.202479	1344.689288	18.152730
43.475180	1328.163809	18.157747
43.346253	1340.340936	18.162765
43.773769	1336.868924	18.167783
43.730445	1333.347735	18.172800
43.155708	1338.199583	18.177818
43.787490	1330.468269	18.182835
43.555857	1341.351444	18.187853
43.512522	1335.395208	18.192871
43.261649	1331.301504	18.197888
43.594081	1340.729332	18.202906
43.516216	1330.702887	18.207923
43.396551	1332.524866	18.212941
43.610196	1323.345415	18.217959
43.599966	1329.749471	18.222976
43.955562	1345.761450	18.227994
44.115060	1346.299361	18.233011
43.691922	1349.461198	18.238029
44.207931	1355.334599	18.243047
44.107890	1362.970519	18.248064
44.227671	1363.620158	18.253082
44.393215	1357.451274	18.258099
44.470062	1358.183266	18.263117
44.254267	1336.486481	18.268135
44.372952	1331.441932	18.273152
44.334086	1346.909633	18.278170
44.769843	1337.084415	18.283187
44.339456	1330.386091	18.288205
44.127010	1328.132994	18.293223
44.303733	1327.090411	18.298240
44.035874	1349.956407	18.303258
44.342486	1342.119642	18.308275
44.459471	1349.458247	18.313293
44.582065	1354.426978	18.318311
44.562827	1349.961271	18.323328
44.233349	1357.087938	18.328346
44.703247	1356.826011	18.333363
44.606693	1373.888556	18.338381
44.818387	1389.734769	18.343399
45.017565	1379.189051	18.348416
44.924889	1384.247180	18.353434
45.258748	1373.130998	18.358451
45.630284	1371.127680	18.363469
45.617853	1368.606723	18.368487
45.340317	1346.064041	18.373504
45.490028	1349.175417	18.378522
45.069500	1332.438020	18.383539
45.105363	1337.651812	18.388557
44.797120	1343.247675	18.393575
45.470213	1355.068817	18.398592
45.428381	1365.223315	18.403610
45.679140	1362.334767	18.408627
45.644683	1356.411713	18.413645
45.315072	1360.057286	18.418663
45.511885	1365.353958	18.423680
45.289509	1372.013665	18.428698
45.754636	1365.502842	18.433715
45.738146	1369.131514	18.438733
45.813276	1376.143325	18.443751
46.042587	1364.074836	18.448768
45.850399	1369.125234	18.453786
45.667797	1376.815227	18.458803
46.152062	1365.826075	18.463821
45.851306	1363.752225	18.468839
45.872362	1370.560298	18.473856
45.814097	1361.482390	18.478874
45.911716	1367.518477	18.483891
45.905463	1366.668668	18.488909
45.905001	1376.660846	18.493927
45.872790	1366.107995	18.498944
45.984215	1372.064804	18.503962
45.896399	1368.531825	18.508979
46.088579	1383.302045	18.513997
46.262415	1396.443967	18.519015
46.578265	1404.038750	18.524032
46.485880	1401.299302	18.529050
46.573081	1398.603574	18.534067
46.554358	1399.486090	18.539085
46.122175	1402.855448	18.544103
46.553199	1397.759490	18.549120
46.430502	1395.589597	18.554138
46.786090	1395.687248	18.559155
46.982855	1397.383264	18.564173
46.833866	1388.466100	18.569191
46.811731	1394.518151	18.574208
46.656379	1398.919314	18.579226
46.833353	1395.049942	18.584243
46.842485	1390.505766	18.589261
46.776778	1403.734662	18.594279
47.109817	1401.223097	18.599296
47.284679	1399.329794	18.604314
47.083926	1392.837065	18.609331
47.090206	1399.968408	18.614349
47.104466	1402.363644	18.619367
47.467533	1409.521461	18.624384
47.527375	1420.084502	18.629402
47.430714	1418.918770	18.634419
47.377652	1401.955946	18.639437
47.234967	1420.262309	18.644455
47.463710	1416.412990	18.649472
47.079955	1419.953954	18.654490
47.427909	1424.266991	18.659507
47.516324	1422.184550	18.664525
47.628965	1421.397574	18.669543
47.508848	1415.318269	18.674560
46.985531	1434.176140	18.679578
47.729195	1437.158203	18.684595
47.916367	1438.679573	18.689613
47.586405	1452.656952	18.694631
48.165868	1437.189848	18.699648
48.540087	1447.068836	18.704666
48.114748	1441.285165	18.709683
47.886985	1435.260771	18.714701
47.919824	1443.831950	18.719719
48.198820	1443.524961	18.724736
47.984631	1454.937127	18.729754
47.973578	1441.747576	18.734771
48.393677	1433.598505	18.739789
48.291458	1449.433499	18.744807
48.383236	1437.352276	18.749824
48.274859	1435.549757	18.754842
48.324759	1451.369932	18.759859
48.291722	1433.485221	18.764877
48.365490	1442.562682	18.769895
48.591240	1437.121919	18.774912
48.355598	1439.357239	18.779930
48.393776	1459.451668	18.784947
49.061694	1465.656396	18.789965
48.850953	1477.970956	18.794983
48.941407	1470.349497	18.800000
48.643220	1468.050276	18.805018
48.945325	1462.155301	18.810035
48.855309	1463.178181	18.815053
48.847095	1462.849356	18.820071
48.814361	1471.475053	18.825088
48.713080	1468.727573	18.830106
48.939372	1468.595732	18.835123
49.240918	1456.191599	18.840141
49.168411	1465.010828	18.845159
49.372000	1449.016911	18.850176
49.354136	1453.501557	18.855194
49.285484	1484.676261	18.860211
49.861522	1485.441906	18.865229
49.659076	1481.510325	18.870247
49.751837	1469.166220	18.875264
49.655764	1468.333876	18.880282
49.539016	1458.371746	18.885299
49.560706	1459.317035	18.890317
49.763802	1477.170344	18.895335
50.005851	1474.006308	18.900352
49.910569	1487.911687	18.905370
49.891350	1478.511297	18.910387
50.444997	1476.431731	18.915405
49.675127	1463.064299	18.920423
49.951346	1471.875108	18.925440
50.013276	1478.049069	18.930458
49.766599	1478.612436	18.935475
50.172015	1475.556055	18.940493
49.949412	1487.452512	18.945511
50.713967	1483.324240	18.950528
50.630752	1485.074356	18.955546
50.315589	1474.166998	18.960563
50.214609	1483.220443	18.965581
50.182829	1486.722593	18.970599
50.277200	1476.844759	18.975616
50.182539	1492.260165	18.980634
49.886337	1485.724414	18.985651
50.707906	1494.509613	18.990669
50.412533	1501.427988	18.995687
50.603816	1510.209894	19.000704
50.500648	1526.255911	19.005722
50.590359	1516.083061	19.010739
50.978849	1514.157246	19.015757
50.849846	1521.536742	19.020775
51.088438	1507.676525	19.025792
51.100052	1507.953306	19.030810
51.068849	1509.355352	19.035827
51.201353	1511.577589	19.040845
51.101873	1509.775215	19.045863
51.441725	1507.990867	19.050880
51.275341	1505.807475	19.055898
50.948504	1499.100423	19.060915
51.302765	1502.452920	19.065933
51.309067	1500.970309	19.070951
51.367703	1501.104309	19.075968
51.508066	1495.096688	19.080986
51.147066	1510.729197	19.086003
51.602696	1491.666922	19.091021
51.399648	1514.385984	19.096039
51.440019	1510.319714	19.101056
51.712696	1531.858656	19.106074
52.120483	1521.540692	19.111091
52.052682	1525.680961	19.116109
51.982185	1516.741762	19.121127
52.212046	1524.694821	19.126144
52.020230	1496.069413	19.131162
51.655136	1500.738440	19.136179
52.185320	1506.022897	19.141197
51.854030	1517.091986	19.146215
52.194979	1528.359046	19.151232
52.060983	1521.234259	19.156250
52.268164	1543.936708	19.161267
52.428605	1516.091946	19.166285
51.969774	1535.290454	19.171303
52.259453	1526.166391	19.176320
52.265049	1524.526585	19.181338
51.912569	1528.471580	19.186355
52.303472	1540.059449	19.191373
52.448914	1552.103333	19.196391
52.683750	1543.938129	19.201408
52.957214	1555.706765	19.206426
52.988107	1554.969000	19.211443
53.365999	1542.142052	19.216461
53.097802	1548.329365	19.221479
53.052726	1525.392248	19.226496
53.300937	1516.578403	19.231514
52.994624	1521.673796	19.236531
53.219991	1513.146745	19.241549
53.156998	1513.677674	19.246567
52.796082	1516.916139	19.251584
52.978065	1520.181283	19.256602
53.101015	1540.559611	19.261619
53.301693	1541.243549	19.266637
53.189097	1553.182292	19.271655
53.338492	1539.622565	19.276672
53.764672	1545.578013	19.281690
53.233402	1550.706146	19.286707
53.611408	1536.480742	19.291725
53.543929	1551.163553	19.296743
53.577289	1546.687825	19.301760
53.652504	1548.673808	19.306778
53.442944	1553.058494	19.311795
53.755629	1549.538679	19.316813
53.497272	1545.719817	19.321831
53.568520	1547.586881	19.326848
53.785611	1556.504701	19.331866
53.963561	1570.785016	19.336883
54.021051	1570.205033	19.341901
54.281653	1575.721276	19.346919
54.284955	1582.461493	19.351936
54.483221	1570.864981	19.356954
53.976803	1581.241589	19.361971
54.154929	1569.511434	19.366989
53.938385	1582.025212	19.372007
54.359275	1571.480177	19.377024
54.427502	1566.891914	19.382042
54.245614	1572.255350	19.387059
54.218795	1571.918478	19.392077
54.232801	1566.118173	19.397095
54.607911	1594.290170	19.402112
54.571544	1608.419080	19.407130
54.582800	1611.689449	19.412147
54.848117	1599.029846	19.417165
54.829846	1604.129669	19.422183
54.751412	1591.276350	19.427200
54.968164	1594.581585	19.432218
54.589516	1605.063677	19.437235
54.785228	1588.756252	19.442253
55.390112	1593.665454	19.447271
55.380907	1621.807557	19.452288
55.406712	1601.808502	19.457306
55.251496	1586.373461	19.462323
55.307566	1597.753650	19.467341
55.455583	1607.126119	19.472359
55.579068	1605.857622	19.477376
56.061804	1609.497975	19.482394
55.683335	1607.445920	19.487411
55.890067	1597.737279	19.492429
55.772614	1591.286233	19.497447
55.733962	1584.356998	19.502464
55.712757	1587.774114	19.507482
55.706793	1593.842546	19.512499
55.998599	1602.348923	19.517517
55.983567	1591.506871	19.522535
55.842496	1609.806923	19.527552
56.174366	1605.423572	19.532570
56.007258	1612.909867	19.537587
56.260612	1604.894262	19.542605
56.156719	1608.546371	19.547623
56.164181	1615.114476	19.552640
56.465625	1610.245182	19.557658
56.296345	1611.213071	19.562675
56.460154	1615.050583	19.567693
56.375643	1605.273551	19.572711
56.371887	1617.803762	19.577728
56.287141	1612.060087	19.582746
56.290383	1610.310533	19.587763
56.309797	1611.028101	19.592781
56.200917	1598.944137	19.597799
56.275210	1617.039962	19.602816
56.574379	1630.330426	19.607834
56.748353	1638.382125	19.612851
56.717577	1631.778808	19.617869
56.985991	1635.274019	19.622887
56.546255	1643.906524	19.627904
56.817671	1630.593100	19.632922
56.823808	1642.846470	19.637939
57.026251	1658.029049	19.642957
57.594053	1659.065014	19.647975
57.288607	1656.702423	19.652992
57.464946	1659.944903	19.658010
57.500634	1661.751585	19.663027
57.761274	1657.412613	19.668045
57.718688	1660.122131	19.673063
57.667330	1655.280772	19.678080
57.968885	1652.700253	19.683098
57.919197	1656.362606	19.688115
57.926859	1650.366645	19.693133
58.413260	1636.208804	19.698151
58.027381	1631.886426	19.703168
58.090515	1620.305134	19.708186
57.786611	1633.993806	19.713203
57.886560	1621.801012	19.718221
58.002269	1622.509517	19.723239
57.888232	1653.789351	19.728256
58.156421	1650.273462	19.733274
58.041254	1656.293267	19.738291
57.869670	1649.715544	19.743309
58.227476	1650.177796	19.748327
58.217592	1653.604134	19.753344
58.494501	1655.266950	19.758362
58.518623	1652.529324	19.763379
58.231315	1658.235227	19.768397
58.561888	1671.762974	19.773415
58.592095	1679.422334	19.778432
58.658883	1681.920926	19.783450
59.106239	1674.207835	19.788467
58.635120	1685.017771	19.793485
58.788309	1677.979244	19.798503
59.094922	1662.835422	19.803520
59.182950	1672.384246	19.808538
59.172788	1675.005223	19.813555
59.450069	1681.011217	19.818573
59.665343	1669.402476	19.823591
59.096623	1677.292633	19.828608
59.270817	1667.851837	19.833626
59.705725	1664.290480	19.838643
59.517002	1671.418448	19.843661
59.833661	1660.671315	19.848679
59.812360	1660.553790	19.853696
59.719025	1640.848967	19.858714
59.622196	1638.698507	19.863731
59.479901	1635.553259	19.868749
59.899839	1639.963424	19.873767
59.637824	1672.319275	19.878784
59.603629	1664.764785	19.883802
59.850104	1659.827161	19.888819
59.647555	1673.189813	19.893837
59.683707	1669.390019	19.898855
59.795705	1670.819581	19.903872
59.489393	1670.986614	19.908890
59.839870	1670.300126	19.913907
59.910738	1694.816272	19.918925
60.164813	1679.589574	19.923943
60.021710	1687.476356	19.928960
60.216228	1695.057610	19.933978
59.986064	1699.994625	19.938995
60.254343	1707.383218	19.944013
60.375273	1716.121412	19.949031
60.510255	1728.090031	19.954048
60.854008	1721.656613	19.959066
61.060022	1721.630255	19.964083
60.794274	1724.084356	19.969101
60.947345	1714.775890	19.974119
60.829305	1730.048980	19.979136
61.179923	1725.476982	19.984154
61.389904	1715.761453	19.989171
60.903043	1724.664222	19.994189
61.323005	1729.044523	19.999207
61.217627	1727.584418	20.004224
61.208843	1720.762043	20.009242
61.450566	1715.670998	20.014259
61.027470	1724.815289	20.019277
61.403205	1723.871507	20.024295
61.211966	1736.033733	20.029312
61.523263	1749.354621	20.034330
61.630083	1746.371760	20.039347
61.623759	1750.533751	20.044365
61.748201	1741.693103	20.049383
61.520752	1758.451349	20.054400
61.777258	1753.032306	20.059418
61.763129	1746.950116	20.064435
61.964541	1750.220080	20.069453
62.218737	1739.720385	20.074471
62.013188	1745.363732	20.079488
62.104343	1761.211486	20.084506
62.777696	1761.738255	20.089523
62.419878	1747.983148	20.094541
62.639891	1741.461700	20.099559
62.149323	1737.584647	20.104576
62.391872	1734.923860	20.109594
62.570284	1747.296140	20.114611
62.573173	1752.210950	20.119629
62.763341	1756.581501	20.124647
62.709640	1755.286190	20.129664
62.830266	1765.714730	20.134682
63.148778	1761.980785	20.139699
62.919333	1764.595849	20.144717
62.965019	1773.324054	20.149735
62.849038	1759.728576	20.154752
63.173625	1762.727994	20.159770
63.484786	1755.420411	20.164787
63.162662	1761.141344	20.169805
63.433354	1757.528287	20.174823
63.461789	1755.613458	20.179840
63.368512	1771.371083	20.184858
63.409027	1756.057235	20.189875
63.274521	1757.043970	20.194893
63.157776	1764.221853	20.199911
63.182245	1760.961104	20.204928
63.137479	1771.873789	20.209946
63.312810	1763.171309	20.214963
63.367911	1794.415034	20.219981
63.459338	1786.558079	20.224999
63.762985	1786.958185	20.230016
63.900718	1793.537844	20.235034
63.865536	1781.346804	20.240051
63.810225	1791.073512	20.245069
63.980213	1799.049642	20.250087
64.055569	1814.317149	20.255104
64.114394	1815.398116	20.260122
64.688627	1810.415251	20.265139
64.423535	1816.769715	20.270157
65.060698	1810.843977	20.275175
64.756530	1812.648246	20.280192
64.755222	1807.984476	20.285210
64.898699	1807.087953	20.290227
64.654861	1811.889542	20.295245
64.872153	1803.365183	20.300263
64.510579	1813.683461	20.305280
64.521917	1810.700870	20.310298
64.884342	1812.773226	20.315315
64.687778	1813.379737	20.320333
64.976818	1807.717165	20.325351
64.649938	1808.378280	20.330368
65.104065	1827.218423	20.335386
65.187111	1829.608265	20.340403
64.855738	1835.851393	20.345421
64.935137	1833.959101	20.350439
65.455394	1834.748611	20.355456
65.038384	1840.782807	20.360474
65.577621	1844.691075	20.365491
65.684759	1855.944554	20.370509
65.954204	1865.260858	20.375527
66.010071	1853.660875	20.380544
65.734227	1845.650879	20.385562
66.075755	1848.739639	20.390579
65.911951	1846.297010	20.395597
65.913184	1856.172840	20.400615
65.990796	1859.442122	20.405632
66.202817	1858.907486	20.410650
66.624764	1850.497546	20.415667
66.243212	1859.200338	20.420685
66.631761	1852.349931	20.425703
66.234060	1856.095362	20.430720
66.367000	1866.261665	20.435738
66.710957	1859.542640	20.440755
66.304918	1857.531125	20.445773
66.526599	1854.621164	20.450791
66.612079	1854.552678	20.455808
66.333749	1856.436204	20.460826
66.517219	1863.607160	20.465843
66.537437	1871.690587	20.470861
66.675311	1878.061829	20.475879
66.699066	1883.238421	20.480896
66.747704	1892.400399	20.485914
67.150713	1883.260401	20.490931
66.947527	1887.765297	20.495949
67.208370	1883.145430	20.500967
67.403818	1881.978696	20.505984
67.059858	1896.248178	20.511002
67.730266	1903.728480	20.516019
67.850528	1919.618958	20.521037
67.696658	1911.930834	20.526055
67.807190	1910.686400	20.531072
67.951776	1916.697136	20.536090
68.006882	1907.477319	20.541107
67.590260	1915.363011	20.546125
68.049582	1907.956216	20.551143
68.226334	1903.239637	20.556160
67.738754	1910.741796	20.561178
68.244730	1898.855270	20.566195
67.796519	1904.333661	20.571213
68.351630	1903.826110	20.576231
68.394442	1894.842652	20.581248
68.451795	1910.418310	20.586266
68.396318	1899.549443	20.591283
68.152449	1905.614258	20.596301
68.303385	1909.360302	20.601319
68.352558	1920.165306	20.606336
68.514731	1935.086385	20.611354
68.970118	1932.419936	20.616371
68.805908	1946.524729	20.621389
68.777500	1936.329522	20.626407
69.118736	1930.064737	20.631424
68.793833	1933.846557	20.636442
68.969205	1929.995391	20.641459
69.076489	1927.544125	20.646477
69.075171	1932.703497	20.651495
69.317452	1932.919118	20.656512
69.316742	1945.739362	20.661530
69.854369	1945.984179	20.666547
69.559897	1946.567768	20.671565
69.553267	1932.801312	20.676583
70.017670	1933.644570	20.681600
69.672176	1929.386450	20.686618
69.674063	1916.203055	20.691635
69.812859	1930.989427	20.696653
69.719541	1941.898971	20.701671
70.017420	1947.381097	20.706688
69.951667	1944.726179	20.711706
70.299102	1942.559883	20.716723
69.833917	1940.640375	20.721741
70.050341	1945.706036	20.726759
70.080374	1943.823962	20.731776
70.562431	1939.992316	20.736794
70.302642	1945.649108	20.741811
70.504337	1944.831386	20.746829
70.626685	1937.950243	20.751847
70.378590	1939.375907	20.756864
70.585823	1952.236931	20.761882
70.709964	1961.030606	20.766899
71.015304	1950.307877	20.771917
71.099398	1957.247751	20.776935
71.199243	1957.487661	20.781952
70.907039	1964.438781	20.786970
71.094831	1951.582801	20.791987
71.400473	1955.117775	20.797005
71.112108	1959.929658	20.802023
71.249341	1951.339326	20.807040
71.251617	1958.409444	20.812058
71.438111	1949.973285	20.817075
71.279379	1934.930921	20.822093
71.184990	1962.174087	20.827111
71.798762	1964.765620	20.832128
71.836566	1974.406812	20.837146
71.785810	1989.488539	20.842163
71.504353	1981.379470	20.847181
71.946589	1983.940943	20.852199
71.973349	1983.341461	20.857216
71.734225	1983.432498	20.862234
71.578087	1981.624941	20.867251
71.920627	1986.882087	20.872269
71.897270	2010.720056	20.877287
72.246760	2006.673568	20.882304
72.119759	2006.084448	20.887322
72.094932	2018.662413	20.892339
72.673414	2006.066566	20.897357
72.477646	2012.805694	20.902375
72.800297	2027.356767	20.907392
72.607199	2044.763487	20.912410
72.867849	2036.775586	20.917427
72.914608	2024.266092	20.922445
73.202393	2032.793029	20.927463
73.221626	2035.015322	20.932480
73.110538	2033.609582	20.937498
73.510381	2029.295496	20.942515
73.443574	2024.555581	20.947533
73.125399	2037.743514	20.952551
73.021348	2026.902748	20.957568
73.329842	2031.027199	20.962586
73.447669	2029.772940	20.967603
73.588206	2027.214890	20.972621
73.384433	2031.367548	20.977639
73.734745	2023.629637	20.982656
73.944813	2016.263323	20.987674
73.700361	2019.517931	20.992691
74.136933	2026.993115	20.997709
73.921029	2045.846796	21.002727
74.155161	2036.352156	21.007744
74.187762	2050.199137	21.012762
73.915968	2045.834843	21.017779
74.313986	2038.159320	21.022797
74.041319	2044.926456	21.027815
74.396738	2044.167589	21.032832
74.412992	2048.451126	21.037850
74.541463	2038.426681	21.042867
74.500521	2039.863366	21.047885
74.730902	2070.385993	21.052903
75.051213	2065.195774	21.057920
74.935627	2068.149829	21.062938
75.252244	2064.878604	21.067955
75.193607	2066.150577	21.072973
75.112945	2064.009274	21.077991
75.525976	2070.376048	21.083008
75.356391	2066.864590	21.088026
75.273716	2064.095151	21.093043
75.390567	2070.452525	21.098061
75.536519	2063.371707	21.103079
75.527685	2056.621545	21.108096
75.234678	2067.227956	21.113114
75.310878	2067.739853	21.118131
75.932433	2059.794278	21.123149
75.666775	2066.970887	21.128167
75.972578	2046.981627	21.133184
75.976271	2065.391306	21.138202
76.202221	2092.823531	21.143219
76.353082	2089.340408	21.148237
75.971927	2080.234099	21.153255
76.403883	2088.584700	21.158272
76.494498	2089.327119	21.163290
76.273154	2082.085416	21.168307
76.587436	2087.260584	21.173325
76.421463	2086.857797	21.178343
76.285679	2089.760018	21.183360
76.502704	2098.834709	21.188378
76.629894	2083.398937	21.193395
76.819047	2090.562807	21.198413
76.427407	2098.566528	21.203431
76.717235	2104.009098	21.208448
76.834002	2117.853733	21.213466
76.521577	2116.187493	21.218483
77.004010	2121.630031	21.223501
77.040814	2120.525545	21.228519
77.300279	2127.833960	21.233536
77.606611	2132.797255	21.238554
77.874515	2134.677869	21.243571
77.791067	2125.719122	21.248589
77.686423	2126.805731	21.253607
78.193573	2131.589916	21.258624
78.262797	2131.639645	21.263642
77.923797	2115.055873	21.268659
77.702840	2109.675873	21.273677
77.820906	2119.100644	21.278695
78.016897	2134.298910	21.283712
78.334637	2139.146338	21.288730
78.073627	2138.048443	21.293747
78.298177	2127.142615	21.298765
78.396210	2137.494011	21.303783
78.285434	2127.024711	21.308800
78.682612	2130.451532	21.313818
78.210947	2130.948546	21.318835
78.700422	2142.897159	21.323853
78.585459	2152.260006	21.328871
78.914341	2162.298524	21.333888
78.749253	2155.645597	21.338906
78.962567	2155.636168	21.343923
79.052819	2150.799589	21.348941
78.872755	2149.671480	21.353959
79.477943	2159.191639	21.358976
79.507102	2158.638175	21.363994
79.303994	2155.637798	21.369011
79.464702	2153.181122	21.374029
79.424186	2166.232078	21.379047
79.433095	2171.835882	21.384064
79.610074	2177.833696	21.389082
79.767793	2177.453224	21.394099
79.860821	2173.317020	21.399117
79.996593	2173.083988	21.404135
80.256091	2177.899816	21.409152
80.205812	2182.444915	21.414170
80.100469	2184.586416	21.419187
80.477504	2178.077490	21.424205
80.225504	2174.356551	21.429223
80.189858	2171.443517	21.434240
80.194148	2188.951860	21.439258
80.543803	2203.081928	21.444275
80.940457	2198.728974	21.449293
80.748912	2211.312454	21.454311
81.033567	2212.346426	21.459328
81.286215	2194.435672	21.464346
80.978179	2203.270096	21.469363
80.879455	2201.513921	21.474381
80.998067	2216.246383	21.479399
80.826443	2208.457106	21.484416
81.404765	2207.197042	21.489434
80.784537	2198.572403	21.494451
81.135914	2192.928059	21.499469
81.406896	2208.549413	21.504487
81.357868	2218.554634	21.509504
81.760397	2224.923152	21.514522
81.669713	2235.508432	21.519539
81.698016	2225.215883	21.524557
81.541309	2229.157371	21.529575
81.563208	2231.019809	21.534592
81.869538	2222.513258	21.539610
81.842973	2231.590695	21.544627
82.311415	2232.511986	21.549645
82.203637	2254.280998	21.554663
82.358126	2250.216775	21.559680
82.502073	2247.411948	21.564698
82.423276	2255.925898	21.569715
82.869401	2253.876751	21.574733
82.726908	2253.445044	21.579751
82.394556	2243.937567	21.584768
82.810490	2248.393396	21.589786
82.462132	2258.232432	21.594803
82.721948	2252.763126	21.599821
82.649067	2271.933299	21.604839
82.805721	2271.946277	21.609856
83.304702	2268.292759	21.614874
83.061718	2275.426526	21.619891
83.420237	2277.364287	21.624909
83.811407	2267.844455	21.629927
83.751888	2269.221200	21.634944
83.687945	2269.942655	21.639962
83.471752	2279.401956	21.644979
84.003103	2276.979755	21.649997
84.179494	2294.914629	21.655015
84.196905	2292.541346	21.660032
84.454971	2273.788005	21.665050
83.981945	2271.411131	21.670067
84.092367	2282.617224	21.675085
84.224482	2283.025825	21.680103
84.478801	2289.569027	21.685120
84.810321	2295.634275	21.690138
84.750865	2295.688007	21.695155
84.890070	2285.355707	21.700173
84.537168	2283.678597	21.705191
84.575430	2280.369124	21.710208
84.693459	2286.179743	21.715226
84.795970	2286.074718	21.720243
84.813045	2279.306163	21.725261
85.033800	2288.883780	21.730279
85.224481	2293.750736	21.735296
85.277412	2309.908013	21.740314
84.659734	2301.072106	21.745331
85.264375	2301.651550	21.750349
85.317918	2308.298355	21.755367
85.120690	2307.410514	21.760384
85.537434	2310.652561	21.765402
85.434614	2332.264373	21.770419
85.557175	2341.019988	21.775437
85.845436	2340.284404	21.780455
85.733537	2344.995907	21.785472
85.960713	2335.036535	21.790490
85.762179	2332.449126	21.795507
86.065545	2345.614517	21.800525
86.564578	2362.745278	21.805543
86.518145	2368.818127	21.810560
86.633866	2345.019523	21.815578
86.840625	2363.544285	21.820595
86.732576	2358.743980	21.825613
87.064665	2356.597379	21.830631
86.923369	2346.987788	21.835648
87.287199	2340.893845	21.840666
86.996094	2352.259197	21.845683
87.060068	2348.006445	21.850701
87.325183	2336.974434	21.855719
87.051615	2348.745216	21.860736
87.342305	2344.333607	21.865754
87.376335	2342.533434	21.870771
87.012334	2346.625208	21.875789
87.359069	2343.135174	21.880807
87.380678	2369.964174	21.885824
87.597193	2373.708535	21.890842
87.728767	2368.812595	21.895859
87.768920	2363.865163	21.900877
88.004776	2372.642060	21.905895
87.702437	2367.915996	21.910912
88.219593	2384.575097	21.915930
88.264890	2404.943425	21.920947
88.258871	2396.378822	21.925965
88.833993	2396.338441	21.930983
88.703635	2392.225999	21.936000
89.012882	2394.040276	21.941018
88.813772	2394.769920	21.946035
89.026499	2394.446743	21.951053
89.458266	2383.529705	21.956071
89.051019	2379.561316	21.961088
89.391833	2378.918817	21.966106
89.253294	2372.487302	21.971123
89.305254	2376.628379	21.976141
89.449578	2379.394747	21.981159
89.346504	2376.861326	21.986176
89.574012	2371.312965	21.991194
89.446630	2390.894709	21.996211
89.387636	2380.435061	22.001229
89.815989	2373.464801	22.006247
89.545571	2389.039753	22.011264
89.812303	2386.600740	22.016282
89.750220	2409.024990	22.021299
89.981000	2409.557084	22.026317
90.208654	2409.919777	22.031335
89.856153	2412.517608	22.036352
90.115867	2418.261638	22.041370
90.258799	2410.874370	22.046387
90.165570	2405.686265	22.051405
90.648593	2415.215852	22.056423
90.200956	2438.104354	22.061440
90.981444	2434.711884	22.066458
90.949458	2440.965730	22.071475
90.898762	2432.648135	22.076493
91.039540	2428.525483	22.081511
90.608715	2435.749060	22.086528
90.948311	2429.599952	22.091546
90.882081	2459.534359	22.096563
91.329503	2460.467671	22.101581
91.539846	2461.311364	22.106599
91.593600	2478.678449	22.111616
91.653788	2459.318512	22.116634
92.110546	2452.242217	22.121651
91.938282	2471.151626	22.126669
91.960326	2451.950376	22.131687
92.065583	2455.051777	22.136704
91.997301	2459.888506	22.141722
92.035899	2452.394363	22.146739
92.149960	2467.906515	22.151757
92.576761	2475.565192	22.156775
92.319381	2482.412681	22.161792
92.489642	2483.899894	22.166810
92.249908	2484.859407	22.171827
92.422668	2478.880827	22.176845
92.748706	2478.567110	22.181863
92.608128	2496.065100	22.186880
92.942455	2501.586463	22.191898
92.948876	2507.282823	22.196915
92.942616	2518.702776	22.201933
93.185431	2510.818931	22.206951
92.925002	2516.152759	22.211968
93.435888	2515.365148	22.216986
93.869225	2540.105729	22.222003
93.712254	2539.519791	22.227021
94.296454	2529.438856	22.232039
94.052187	2542.165532	22.237056
94.140520	2532.895973	22.242074
94.354721	2534.032449	22.247091
94.064117	2524.993222	22.252109
94.210219	2523.845321	22.257127
94.227135	2533.262107	22.262144
94.481924	2535.444554	22.267162
94.569328	2525.128997	22.272179
94.392559	2538.595303	22.277197
94.843726	2513.025831	22.282215
94.125706	2527.390971	22.287232
94.130726	2520.494441	22.292250
94.533043	2540.732876	22.297267
94.500445	2550.364439	22.302285
94.886590	2544.829259	22.307303
94.907921	2558.592784	22.312320
94.967051	2555.554438	22.317338
95.112065	2569.546023	22.322355
95.146173	2578.666702	22.327373
95.760925	2571.358286	22.332391
95.948511	2573.582132	22.337408
95.954286	2582.709691	22.342426
95.605513	2579.635703	22.347443
95.601118	2574.741712	22.352461
95.848044	2575.351470	22.357479
95.918477	2583.392677	22.362496
96.137322	2605.703212	22.367514
96.298271	2606.590973	22.372531
96.439120	2603.596220	22.377549
96.905279	2598.243334	22.382567
96.641937	2605.526810	22.387584
96.801201	2602.837462	22.392602
97.010824	2592.522033	22.397619
96.853088	2604.125884	22.402637
97.174413	2601.158200	22.407655
96.848934	2602.028351	22.412672
96.824211	2599.727810	22.417690
96.936379	2600.946635	22.422707
97.015968	2607.380193	22.427725
97.140001	2612.696798	22.432743
97.030471	2626.067511	22.437760
97.624434	2619.611897	22.442778
97.681985	2626.325069	22.447795
97.781729	2648.823778	22.452813
98.477272	2641.757298	22.457831
98.508237	2643.378435	22.462848
98.207700	2628.527866	22.467866
98.200646	2622.755668	22.472883
98.350162	2638.517989	22.477901
98.483582	2645.555729	22.482919
98.385489	2644.048747	22.487936
98.841364	2648.157742	22.492954
98.921667	2646.151934	22.497971
98.665847	2646.937827	22.502989
98.981771	2642.349058	22.508007
98.781565	2641.038487	22.513024
98.654039	2641.204544	22.518042
98.852069	2644.778875	22.523059
99.141961	2658.784413	22.528077
99.382604	2657.886505	22.533095
99.576828	2673.361710	22.538112
99.364299	2658.834521	22.543130
99.721249	2660.763934	22.548147
99.443641	2670.033488	22.553165
99.587469	2668.660974	22.558183
99.859827	2671.218988	22.563200
99.924754	2680.248293	22.568218
100.124603	2692.107467	22.573235
100.149071	2704.798511	22.578253
100.071144	2687.451936	22.583271
99.917942	2698.313387	22.588288
99.858602	2685.916994	22.593306
100.328580	2714.039860	22.598323
100.447357	2722.419533	22.603341
100.490220	2719.504096	22.608359
100.600526	2717.417981	22.613376
100.668798	2720.153280	22.618394
100.955847	2727.434790	22.623411
101.022704	2740.899402	22.628429
101.135539	2744.792540	22.633447
101.052713	2738.547053	22.638464
101.213468	2747.096243	22.643482
101.570640	2741.338285	22.648499
101.328532	2744.643019	22.653517
101.661719	2759.284394	22.658535
101.993065	2765.678664	22.663552
101.805836	2761.866224	22.668570
102.030610	2770.302963	22.673587
101.878192	2762.804510	22.678605
102.569679	2764.369102	22.683623
102.381336	2758.565978	22.688640
102.513297	2769.046921	22.693658
102.792552	2757.485324	22.698675
102.666058	2754.855673	22.703693
102.580801	2789.083070	22.708711
102.639161	2792.122015	22.713728
102.836119	2791.198029	22.718746
103.045316	2796.258064	22.723763
103.034237	2791.679704	22.728781
103.161331	2800.950879	22.733799
103.389329	2800.828201	22.738816
103.516033	2809.465450	22.743834
103.927032	2812.915405	22.748851
104.000794	2819.599337	22.753869
104.129191	2817.087135	22.758887
104.289179	2815.766307	22.763904
104.392633	2803.217214	22.768922
104.197512	2792.963038	22.773939
103.999924	2797.483049	22.778957
104.151902	2800.940481	22.783975
104.403511	2800.611097	22.788992
104.144275	2817.594296	22.794010
104.495971	2799.296522	22.799027
104.477248	2807.525907	22.804045
104.742414	2807.505852	22.809063
105.052834	2827.221311	22.814080
104.952324	2834.274421	22.819098
105.013731	2832.698722	22.824115
104.923836	2845.744787	22.829133
105.117784	2838.348383	22.834151
105.489385	2834.047223	22.839168
105.465467	2839.108262	22.844186
105.512989	2835.268595	22.849203
105.384448	2848.000681	22.854221
105.519135	2866.620956	22.859239
105.950482	2860.099138	22.864256
105.711952	2870.233348	22.869274
105.766800	2862.651451	22.874291
105.807463	2865.524115	22.879309
105.926165	2877.704727	22.884327
106.474058	2887.149556	22.889344
106.239254	2890.410680	22.894362
106.641417	2882.733274	22.899379
106.639843	2883.375593	22.904397
106.556456	2885.331990	22.909415
106.808900	2888.649926	22.914432
106.836868	2904.626993	22.919450
107.232686	2907.792283	22.924467
107.127892	2921.333989	22.929485
107.202407	2906.030817	22.934503
107.424542	2913.574484	22.939520
107.337173	2915.432408	22.944538
107.592737	2925.063105	22.949555
107.599447	2934.002738	22.954573
107.697863	2932.769591	22.959591
108.037289	2944.115089	22.964608
108.371946	2935.705082	22.969626
108.363735	2941.496764	22.974643
108.428876	2937.945303	22.979661
108.182995	2935.908875	22.984679
108.391455	2932.287367	22.989696
108.465647	2942.002844	22.994714
108.585270	2950.337678	22.999731
108.739756	2959.815397	23.004749
108.923279	2960.863981	23.009767
108.991487	2958.797131	23.014784
108.811105	2969.125080	23.019802
109.150880	2961.549614	23.024819
109.208458	2990.306701	23.029837
109.405219	2989.695803	23.034855
109.478266	2977.843620	23.039872
109.495132	2987.340155	23.044890
109.708769	2983.236407	23.049907
109.811431	2980.478929	23.054925
109.998653	3002.906813	23.059943
110.373148	3000.374218	23.064960
110.241047	3012.360526	23.069978
110.767634	3018.546790	23.074995
110.673833	3009.296532	23.080013
110.701024	3008.055858	23.085031
111.054787	3000.143048	23.090048
110.918398	3005.133979	23.095066
110.845098	2999.162959	23.100083
110.860011	2999.353503	23.105101
110.849052	2994.590207	23.110119
111.259171	2984.690897	23.115136
111.007324	3010.083506	23.120154
111.110820	3002.383654	23.125171
111.526877	3027.641474	23.130189
111.601096	3017.695804	23.135207
111.944395	3028.093679	23.140224
111.693325	3030.231008	23.145242
111.710432	3022.190948	23.150259
111.877212	3028.990721	23.155277
111.807082	3024.347762	23.160295
112.148633	3032.489934	23.165312
112.143625	3048.145975	23.170330
112.205604	3039.574871	23.175347
112.220158	3051.347467	23.180365
112.365830	3049.656050	23.185383
112.922765	3056.481723	23.190400
112.643998	3078.503411	23.195418
113.077254	3072.803988	23.200435
113.092732	3073.364935	23.205453
113.128407	3077.665344	23.210471
113.191345	3072.548851	23.215488
113.379410	3094.934266	23.220506
113.327266	3094.927839	23.225523
113.591828	3095.850240	23.230541
113.617661	3104.024703	23.235559
113.928686	3098.328243	23.240576
113.520179	3113.323439	23.245594
114.002003	3116.215481	23.250611
114.223951	3127.740324	23.255629
114.004479	3139.639195	23.260647
114.478812	3134.261217	23.265664
114.641275	3127.983529	23.270682
114.636920	3125.478285	23.275699
114.637074	3134.540224	23.280717
114.642483	3150.358328	23.285735
115.218639	3151.378144	23.290752
114.934057	3153.993588	23.295770
115.387545	3159.352254	23.300787
115.466880	3153.923194	23.305805
115.267195	3154.236845	23.310823
115.513768	3149.305004	23.315840
115.683854	3175.632763	23.320858
116.010350	3182.071256	23.325875
116.153569	3174.291039	23.330893
116.201842	3186.488645	23.335911
116.433009	3181.597793	23.340928
116.319087	3185.656211	23.345946
116.610316	3187.884866	23.350963
116.495862	3175.577867	23.355981
116.378993	3182.873669	23.360999
116.461705	3184.594382	23.366016
116.841324	3198.855943	23.371034
116.939006	3213.462960	23.376051
117.039373	3210.511511	23.381069
116.933059	3215.306570	23.386087
117.203093	3210.401645	23.391104
117.079928	3212.518605	23.396122
117.091375	3226.547065	23.401139
117.314172	3234.341723	23.406157
117.518364	3239.660722	23.411175
117.618980	3228.972853	23.416192
117.876598	3240.429956	23.421210
117.759111	3249.887514	23.426227
118.490756	3253.288809	23.431245
118.488931	3261.669145	23.436263
118.681389	3262.692729	23.441280
118.460440	3259.646980	23.446298
118.423615	3262.184393	23.451315
118.814930	3267.318601	23.456333
119.010589	3257.361271	23.461351
118.770443	3253.963820	23.466368
118.825166	3260.070466	23.471386
119.066811	3284.693423	23.476403
119.222163	3280.612260	23.481421
118.998887	3290.902437	23.486439
119.115313	3284.473127	23.491456
119.260060	3301.365724	23.496474
119.409599	3301.186332	23.501491
119.547053	3316.864782	23.506509
119.709502	3313.070381	23.511527
119.940246	3334.588008	23.516544
120.124198	3343.595598	23.521562
120.229444	3328.348441	23.526579
120.648560	3330.618870	23.531597
120.796174	3339.492232	23.536615
121.000892	3353.836111	23.541632
121.367280	3351.367680	23.546650
121.333186	3364.483971	23.551667
121.693065	3354.707273	23.556685
121.357797	3350.690947	23.561703
121.175392	3351.793976	23.566720
121.393087	3350.156331	23.571738
121.570844	3347.702246	23.576755
122.012970	3355.592577	23.581773
121.696609	3352.366153	23.586791
122.118448	3354.198002	23.591808
122.038475	3338.701903	23.596826
122.171542	3358.577728	23.601843
122.050396	3363.762219	23.606861
122.164699	3378.950427	23.611879
122.281943	3374.965776	23.616896
122.525851	3380.224217	23.621914
122.408307	3394.669078	23.626931
122.733483	3401.904730	23.631949
122.636599	3414.485160	23.636967
122.745568	3414.451470	23.641984
123.148049	3417.406570	23.647002
122.995043	3440.197734	23.652019
123.534169	3433.596337	23.657037
123.305729	3439.435917	23.662055
123.933180	3438.842071	23.667072
124.244136	3445.552186	23.672090
124.279756	3448.715248	23.677107
124.404382	3428.640507	23.682125
124.201726	3437.115896	23.687143
124.650417	3437.525185	23.692160
124.777510	3446.832171	23.697178
124.510062	3452.894299	23.702195
124.980651	3440.978354	23.707213
124.879074	3456.986906	23.712231
125.189756	3442.035686	23.717248
125.349802	3448.024928	23.722266
125.178925	3442.692294	23.727283
125.526634	3437.877171	23.732301
125.244210	3445.776100	23.737319
125.324903	3437.070413	23.742336
125.444071	3446.120648	23.747354
125.124364	3471.255847	23.752371
125.512564	3467.648814	23.757389
125.354128	3477.810788	23.762407
125.828678	3491.790833	23.767424
126.222800	3497.611405	23.772442
126.255617	3505.022734	23.777459
126.633748	3500.729782	23.782477
126.430334	3512.801026	23.787495
126.718923	3520.290361	23.792512
127.025952	3528.052868	23.797530
127.045914	3536.542376	23.802547
127.141294	3531.344248	23.807565
127.363214	3522.094454	23.812583
127.042333	3536.736283	23.817600
127.034300	3533.669899	23.822618
127.256914	3557.712670	23.827635
127.610895	3548.310435	23.832653
128.041451	3563.949495	23.837671
127.876931	3577.191396	23.842688
128.162821	3583.867813	23.847706
128.422959	3589.085197	23.852723
128.358705	3576.751763	23.857741
128.479970	3583.855614	23.862759
128.560150	3578.382997	23.867776
128.736383	3594.200302	23.872794
128.739135	3591.965234	23.877811
129.130389	3604.600148	23.882829
129.280577	3598.547623	23.887847
129.175633	3608.612269	23.892864
129.759572	3589.350611	23.897882
129.404153	3606.022029	23.902899
129.755452	3623.997516	23.907917
130.204459	3638.677949	23.912935
129.900794	3628.450718	23.917952
130.044125	3622.976668	23.922970
130.228234	3630.542504	23.927987
130.369620	3620.655727	23.933005
130.287480	3618.246184	23.938023
130.435784	3640.810263	23.943040
130.997819	3646.158885	23.948058
130.925029	3656.569277	23.953075
131.055993	3648.980343	23.958093
131.156931	3642.725620	23.963111
131.076598	3646.166018	23.968128
131.392479	3641.759450	23.973146
130.952368	3641.998956	23.978163
131.417572	3660.358298	23.983181
131.355900	3673.550061	23.988199
131.238229	3672.229378	23.993216
132.307847	3669.052495	23.998234
132.097720	3670.427425	24.003251
132.203932	3675.810979	24.008269
132.185119	3689.076946	24.013287
132.227502	3699.170081	24.018304
132.561107	3689.993625	24.023322
132.309358	3696.777845	24.028339
132.869072	3708.108484	24.033357
133.242864	3723.912522	24.038375
133.185023	3721.485715	24.043392
133.742080	3720.900726	24.048410
133.453179	3728.772520	24.053427
133.510499	3713.780397	24.058445
133.734936	3712.998291	24.063463
133.893830	3721.977072	24.068480
133.988631	3707.849793	24.073498
134.037820	3730.939559	24.078515
134.139603	3739.354780	24.083533
134.463258	3740.354334	24.088551
134.404408	3744.361646	24.093568
134.796034	3739.283764	24.098586
134.658137	3733.029325	24.103603
134.448380	3746.106316	24.108621
134.286520	3761.439645	24.113639
134.783428	3771.033995	24.118656
135.041860	3776.403542	24.123674
135.180558	3803.716812	24.128691
135.642815	3800.802728	24.133709
135.717914	3806.715198	24.138727
135.705765	3803.751678	24.143744
136.002277	3805.402189	24.148762
136.073337	3814.981084	24.153779
136.004770	3822.670693	24.158797
136.365227	3837.838222	24.163815
136.339303	3833.664666	24.168832
136.526076	3837.208050	24.173850
136.505260	3828.975359	24.178867
136.906571	3837.447502	24.183885
137.125218	3851.580401	24.188903
136.977864	3855.971580	24.193920
137.406387	3852.656953	24.198938
137.221060	3848.338893	24.203955
137.509757	3852.020999	24.208973
137.756506	3866.512863	24.213991
137.657919	3879.203307	24.219008
137.734625	3876.549705	24.224026
138.082683	3879.843187	24.229043
138.014624	3886.761043	24.234061
138.338045	3872.181802	24.239079
138.221030	3880.897092	24.244096
138.477807	3890.010620	24.249114
138.390175	3899.595993	24.254131
138.581533	3896.197240	24.259149
138.716240	3889.082724	24.264167
139.089734	3913.950822	24.269184
139.698361	3918.685608	24.274202
139.363578	3927.357769	24.279219
139.447533	3930.897116	24.284237
139.804229	3921.110325	24.289255
139.886243	3931.271246	24.294272
139.739279	3928.932560	24.299290
139.797680	3929.480403	24.304307
139.905905	3946.543194	24.309325
140.311239	3950.163461	24.314343
140.444012	3949.661062	24.319360
140.723096	3947.064859	24.324378
140.477660	3961.435483	24.329395
140.797837	3976.314583	24.334413
141.513326	3976.175534	24.339431
141.265993	3975.016309	24.344448
141.253717	3969.791139	24.349466
141.337561	3979.633206	24.354483
141.643178	3974.867888	24.359501
141.707906	3992.819509	24.364519
141.828162	4002.696693	24.369536
142.249911	3996.176698	24.374554
142.299031	4004.654748	24.379571
142.393101	4008.817894	24.384589
142.472973	3994.011475	24.389607
142.412117	4005.959700	24.394624
142.938988	4019.275052	24.399642
142.888305	4026.850210	24.404659
142.827223	4026.873526	24.409677
143.223129	4022.708965	24.414695
142.908966	4038.156545	24.419712
143.325310	4039.829671	24.424730
143.728526	4058.942007	24.429747
143.734076	4057.375870	24.434765
143.998376	4040.386121	24.439783
144.002316	4053.528431	24.444800
144.179246	4057.280329	24.449818
144.385316	4067.179273	24.454835
143.960380	4078.710465	24.459853
144.451823	4080.694940	24.464871
144.270333	4084.041435	24.469888
144.400119	4097.885088	24.474906
144.787148	4103.498572	24.479923
144.500897	4106.091632	24.484941
145.434395	4115.488375	24.489959
145.349176	4127.544423	24.494976
145.397904	4134.166082	24.499994
145.699582	4135.382357	24.505011
146.023385	4128.839374	24.510029
146.253556	4124.309451	24.515047
146.415801	4139.276045	24.520064
146.455004	4118.616902	24.525082
146.634192	4122.634351	24.530099
146.290360	4140.083322	24.535117
146.172073	4142.128836	24.540135
146.474155	4146.415402	24.545152
146.725907	4147.220345	24.550170
146.757831	4167.033941	24.555187
146.666902	4176.699474	24.560205
147.530283	4179.489208	24.565223
147.258827	4182.967283	24.570240
148.052691	4192.946448	24.575258
148.215851	4196.714738	24.580275
147.967108	4211.167946	24.585293
148.656422	4196.766048	24.590311
148.391938	4212.986265	24.595328
148.396464	4206.837141	24.600346
148.418966	4200.442861	24.605363
148.521486	4194.263958	24.610381
149.002687	4204.430650	24.615399
149.002791	4231.972136	24.620416
149.457894	4220.342023	24.625434
149.525071	4223.549782	24.630451
149.294807	4229.629898	24.635469
149.361674	4225.944905	24.640487
149.477820	4233.473116	24.645504
149.767926	4241.195437	24.650522
149.827592	4233.700171	24.655539
149.822838	4247.746351	24.660557
149.963548	4247.500706	24.665575
149.883729	4284.495876	24.670592
150.292629	4272.946249	24.675610
150.644105	4294.420867	24.680627
150.605498	4307.005356	24.685645
151.059679	4298.008328	24.690663
151.255051	4303.277204	24.695680
151.248856	4321.961130	24.700698
151.443908	4336.302794	24.705715
151.510750	4332.657112	24.710733
151.972580	4326.796897	24.715751
151.767614	4343.615868	24.720768
152.251498	4350.962000	24.725786
152.669614	4354.903658	24.730803
152.361308	4358.988670	24.735821
152.390362	4358.616077	24.740839
152.676663	4356.165762	24.745856
152.532120	4373.445565	24.750874
153.297197	4374.336240	24.755891
153.299891	4383.231770	24.760909
153.393501	4381.971737	24.765927
153.671527	4383.472649	24.770944
153.465983	4377.851768	24.775962
153.897673	4389.450371	24.780979
153.929155	4400.122362	24.785997
154.356151	4406.566618	24.791015
154.732719	4398.629762	24.796032
154.513836	4399.722161	24.801050
154.625618	4396.693921	24.806067
154.427359	4394.755104	24.811085
154.982220	4391.499673	24.816103
154.919268	4406.615727	24.821120
154.718662	4404.552201	24.826138
155.255996	4422.948206	24.831155
155.058644	4435.583288	24.836173
155.423518	4433.098406	24.841191
155.531860	4436.510478	24.846208
155.727574	4455.993904	24.851226
155.698052	4453.584487	24.856243
155.856619	4464.326731	24.861261
156.089137	4466.081926	24.866279
156.024412	4493.698747	24.871296
156.022226	4496.492815	24.876314
156.369311	4501.335578	24.881331
156.472925	4515.592089	24.886349
156.778203	4516.300411	24.891367
157.259868	4538.079531	24.896384
157.213235	4544.419211	24.901402
157.716371	4549.618653	24.906419
157.745051	4553.495800	24.911437
157.772467	4544.565880	24.916455
158.053692	4557.184551	24.921472
158.262478	4574.045593	24.926490
158.789446	4562.773499	24.931507
158.402659	4575.324047	24.936525
158.852116	4569.843321	24.941543
158.863675	4565.307998	24.946560
158.933162	4582.199125	24.951578
159.560369	4587.143580	24.956595
159.445395	4593.965405	24.961613
159.821603	4595.185572	24.966631
159.781533	4594.031797	24.971648
159.711616	4596.386696	24.976666
160.159591	4589.477571	24.981683
159.823008	4599.571958	24.986701
160.259727	4614.626654	24.991719
160.350447	4618.978528	24.996736
160.348167	4620.688575	25.001754
160.372851	4617.125066	25.006771
160.723329	4656.105829	25.011789
161.227653	4648.483603	25.016807
161.286216	4654.934790	25.021824
161.119804	4652.578633	25.026842
161.388036	4662.811068	25.031859
161.541640	4666.359943	25.036877
161.654532	4678.835632	25.041895
161.788449	4680.313137	25.046912
162.204460	4687.490897	25.051930
162.261071	4698.127630	25.056947
162.593077	4708.664607	25.061965
162.392722	4701.294736	25.066983
162.493915	4695.916692	25.072000
162.595352	4709.798484	25.077018
162.974474	4721.339650	25.082035
163.075104	4720.495419	25.087053
163.209508	4722.464536	25.092071
163.422919	4736.011462	25.097088
163.628590	4752.698559	25.102106
163.501964	4753.858091	25.107123
163.472323	4752.852113	25.112141
163.897040	4772.614128	25.117159
164.462891	4779.760962	25.122176
164.086718	4787.247586	25.127194
164.517477	4790.496626	25.132211
164.869133	4793.354701	25.137229
164.866705	4807.559172	25.142247
165.241816	4815.371303	25.147264
164.925028	4813.858051	25.152282
165.362789	4815.089665	25.157299
165.641726	4845.925033	25.162317
165.891743	4831.008041	25.167335
166.362008	4819.806156	25.172352
166.356246	4836.608089	25.177370
166.843483	4832.822096	25.182387
166.501490	4848.633695	25.187405
166.715384	4863.910622	25.192423
166.944119	4850.568839	25.197440
167.058082	4851.612136	25.202458
167.104925	4857.421757	25.207475
167.181581	4874.500887	25.212493
167.351988	4874.687119	25.217511
167.877518	4877.918709	25.222528
167.712155	4893.592844	25.227546
168.144566	4883.312672	25.232563
168.361146	4895.752346	25.237581
168.458594	4910.777261	25.242599
168.739737	4908.832746	25.247616
168.323454	4908.361211	25.252634
168.720365	4907.699451	25.257651
168.755555	4927.483656	25.262669
169.045558	4936.654691	25.267687
169.249855	4938.259462	25.272704
169.132529	4944.951230	25.277722
169.384706	4956.220952	25.282739
169.500492	4966.776068	25.287757
169.505403	4980.904012	25.292775
170.105897	4990.815435	25.297792
170.180644	4993.612280	25.302810
170.596224	4989.213811	25.307827
170.946455	4994.256849	25.312845
170.917720	4998.010313	25.317863
171.315824	4998.007623	25.322880
171.384591	5014.773488	25.327898
171.596066	5022.685771	25.332915
171.819614	5014.759609	25.337933
171.778561	5013.864000	25.342951
172.168882	5014.613861	25.347968
171.837069	5010.071781	25.352986
172.178488	5003.930764	25.358003
172.340779	5012.743800	25.363021
172.247886	5030.267886	25.368039
172.810263	5029.236734	25.373056
172.667388	5050.093461	25.378074
172.751602	5038.548590	25.383091
172.860563	5052.087286	25.388109
173.057270	5070.108867	25.393127
173.726997	5064.721865	25.398144
173.464621	5067.857263	25.403162
173.870263	5065.032999	25.408179
173.926457	5077.537734	25.413197
173.719318	5077.965893	25.418215
174.431038	5067.857411	25.423232
174.057128	5090.278829	25.428250
174.325133	5108.256835	25.433267
174.496944	5116.147956	25.438285
174.774584	5126.892156	25.443303
175.037252	5134.552455	25.448320
174.995725	5145.416785	25.453338
175.249677	5161.376802	25.458355
175.466308	5167.622067	25.463373
175.707521	5170.980086	25.468391
175.792922	5172.363890	25.473408
175.968469	5189.321411	25.478426
176.462431	5186.444495	25.483443
176.657932	5192.803282	25.488461
176.622208	5205.918328	25.493479
176.910897	5209.746328	25.498496
177.300181	5219.451631	25.503514
177.576731	5214.677180	25.508531
177.544708	5217.277101	25.513549
177.774456	5239.239038	25.518567
178.234621	5234.813721	25.523584
178.224302	5242.568736	25.528602
178.428753	5248.869476	25.533619
178.844032	5247.419624	25.538637
178.346754	5249.362071	25.543655
178.829124	5254.244884	25.548672
178.826991	5271.684768	25.553690
179.049327	5272.975158	25.558707
179.394553	5268.456441	25.563725
179.347157	5280.848841	25.568743
179.731808	5285.316118	25.573760
179.837572	5291.436715	25.578778
179.759574	5290.067074	25.583795
180.333411	5290.127631	25.588813
180.073748	5306.312088	25.593831
180.600834	5313.398496	25.598848
180.702818	5319.112969	25.603866
180.526877	5328.701548	25.608883
181.002542	5324.122683	25.613901
180.808772	5337.408588	25.618919
181.108960	5344.688532	25.623936
181.170640	5352.568229	25.628954
181.340801	5366.653676	25.633971
181.594840	5373.910309	25.638989
181.873567	5376.894992	25.644007
182.311231	5377.133819	25.649024
182.396464	5405.775580	25.654042
182.503363	5401.590631	25.659059
182.718192	5404.448615	25.664077
182.750216	5408.176761	25.669095
183.178534	5412.762206	25.674112
183.780380	5420.721037	25.679130
183.560187	5429.859644	25.684148
183.801916	5432.458443	25.689165
183.733660	5427.368344	25.694183
183.771579	5440.573347	25.699200
184.188029	5458.237024	25.704218
184.366879	5456.708409	25.709236
184.643226	5453.490865	25.714253
184.484738	5472.217050	25.719271
184.691411	5484.982939	25.724288
184.998402	5480.741679	25.729306
185.037471	5504.475459	25.734324
185.395633	5511.059421	25.739341
185.494515	5514.116075	25.744359
185.914931	5517.189128	25.749376
185.864775	5533.760551	25.754394
186.345006	5530.882614	25.759412
186.773933	5535.790565	25.764429
186.657452	5548.541941	25.769447
186.955206	5544.804863	25.774464
187.183590	5566.406392	25.779482
186.860544	5570.611306	25.784500
187.296743	5571.866842	25.789517
187.555824	5586.230204	25.794535
188.155129	5593.161263	25.799552
188.172560	5596.911452	25.804570
187.818870	5600.910413	25.809588
188.708459	5585.268386	25.814605
188.611590	5597.757054	25.819623
188.775789	5602.482223	25.824640
188.924719	5611.935798	25.829658
189.039985	5614.716860	25.834676
189.301428	5615.687923	25.839693
189.396145	5626.287782	25.844711
189.584771	5635.728750	25.849728
189.551527	5651.218193	25.854746
189.778637	5648.987169	25.859764
190.204113	5665.275998	25.864781
190.231469	5678.534037	25.869799
190.340911	5679.096626	25.874816
190.417689	5683.742135	25.879834
190.787568	5697.140697	25.884852
191.144120	5696.370478	25.889869
191.061569	5699.433279	25.894887
190.901501	5711.951000	25.899904
191.401129	5716.528321	25.904922
191.537148	5722.232017	25.909940
191.850679	5728.967955	25.914957
191.915479	5748.081377	25.919975
192.371515	5749.987557	25.924992
192.659112	5751.840342	25.930010
192.748675	5764.116902	25.935028
192.836783	5778.597399	25.940045
192.990039	5782.731159	25.945063
193.355229	5779.928163	25.950080
193.299986	5787.020311	25.955098
193.497522	5802.608443	25.960116
194.037380	5799.017593	25.965133
194.002648	5804.487340	25.970151
194.388734	5827.709214	25.975168
194.899323	5825.517154	25.980186
194.848197	5830.053286	25.985204
194.948054	5823.052756	25.990221
195.017142	5835.672519	25.995239
195.341202	5837.514782	26.000256
195.658218	5848.803177	26.005274
195.795011	5845.976786	26.010292
196.286342	5850.879617	26.015309
196.194807	5857.732903	26.020327
196.059226	5855.230018	26.025344
196.536772	5866.295360	26.030362
196.511167	5872.662154	26.035380
196.701131	5882.548372	26.040397
197.019455	5899.222746	26.045415
197.395473	5905.803254	26.050432
197.326234	5910.782096	26.055450
197.170795	5913.820371	26.060468
197.622874	5919.295949	26.065485
197.923784	5927.995385	26.070503
197.455485	5935.011050	26.075520
197.794159	5945.402306	26.080538
198.318108	5965.943953	26.085556
198.498012	5986.165976	26.090573
198.482118	5990.092306	26.095591
198.842310	6002.249604	26.100608
199.082071	6006.646578	26.105626
199.463342	6029.823120	26.110644
199.829685	6028.982089	26.115661
200.083913	6050.735987	26.120679
200.229415	6043.311090	26.125696
200.680629	6045.203919	26.130714
200.645798	6049.594328	26.135732
200.970223	6066.859569	26.140749
200.933761	6068.811263	26.145767
201.354894	6074.555401	26.150784
201.321889	6066.359593	26.155802
201.639536	6096.351928	26.160820
202.005968	6090.476342	26.165837
202.296647	6103.647150	26.170855
202.184517	6111.013664	26.175872
202.280352	6099.070367	26.180890
202.297566	6111.743481	26.185908
202.575372	6112.508984	26.190925
202.788369	6129.239748	26.195943
202.477327	6140.973098	26.200960
203.017354	6139.638604	26.205978
203.071941	6165.645531	26.210996
203.716523	6161.769612	26.216013
203.693938	6178.287007	26.221031
203.883065	6190.684948	26.226048
204.392234	6188.245231	26.231066
204.536201	6200.336457	26.236084
204.737884	6208.440553	26.241101
204.776928	6207.677655	26.246119
205.154494	6207.036240	26.251136
205.631394	6220.358425	26.256154
205.419881	6234.700668	26.261172
205.782473	6233.432218	26.266189
206.360058	6234.124762	26.271207
206.410846	6243.797376	26.276224
206.620795	6243.062305	26.281242
206.871357	6256.891098	26.286260
207.166341	6250.055169	26.291277
207.255309	6248.520348	26.296295
207.385434	6254.587895	26.301312
207.434910	6249.066472	26.306330
207.516190	6275.136212	26.311348
207.540918	6278.880690	26.316365
207.686103	6281.768833	26.321383
207.779638	6308.908272	26.326400
208.192097	6304.509135	26.331418
208.411709	6321.050235	26.336436
208.660099	6336.947111	26.341453
208.728441	6348.255864	26.346471
209.204707	6358.876463	26.351488
209.639296	6356.547744	26.356506
209.420023	6367.909442	26.361524
209.615531	6375.560641	26.366541
210.323470	6388.658893	26.371559
210.372977	6397.821189	26.376576
210.478211	6394.964320	26.381594
210.464053	6413.442091	26.386612
211.058544	6413.100473	26.391629
211.104600	6416.444258	26.396647
211.640394	6427.712385	26.401664
211.701415	6435.386627	26.406682
211.608977	6442.363853	26.411700
211.879191	6442.388644	26.416717
212.245137	6445.883646	26.421735
212.136339	6473.965957	26.426752
212.595053	6469.467344	26.431770
212.565491	6472.006509	26.436788
212.602421	6490.405420	26.441805
212.737529	6497.523425	26.446823
212.712395	6511.764625	26.451840
213.086714	6524.670704	26.456858
213.213964	6530.193576	26.461876
213.629047	6552.529188	26.466893
214.211233	6559.804910	26.471911
214.328255	6555.049958	26.476928
214.651176	6563.600705	26.481946
214.721209	6587.081086	26.486964
215.158550	6587.974610	26.491981
215.338352	6593.659863	26.496999
215.673706	6611.608512	26.502016
215.970051	6615.013940	26.507034
215.610798	6618.734742	26.512052
215.484505	6626.678130	26.517069
216.148620	6638.715908	26.522087
216.295716	6655.906249	26.527104
216.909434	6662.069970	26.532122
217.153189	6675.196054	26.537140
217.051876	6682.111076	26.542157
217.509456	6681.812524	26.547175
217.653332	6696.518709	26.552192
218.198352	6692.623124	26.557210
218.175525	6693.549098	26.562228
218.203971	6702.711006	26.567245
218.411731	6713.915199	26.572263
218.911108	6719.032627	26.577280
219.165457	6709.976315	26.582298
218.978585	6736.051059	26.587316
219.451075	6743.857356	26.592333
219.852937	6738.384222	26.597351
219.566264	6767.145342	26.602368
219.905434	6775.644841	26.607386
219.994571	6784.915145	26.612404
220.255159	6789.729977	26.617421
220.776766	6795.547294	26.622439
221.027070	6806.127918	26.627456
220.865707	6819.325792	26.632474
221.214771	6832.480864	26.637492
221.364342	6841.020853	26.642509
221.777113	6848.488957	26.647527
221.865767	6864.629024	26.652544
222.233400	6863.156725	26.657562
222.411512	6881.237775	26.662580
222.364839	6892.514134	26.667597
222.501302	6889.001500	26.672615
222.520625	6916.898994	26.677632
222.753295	6932.106621	26.682650
223.071184	6953.223035	26.687668
223.171842	6958.544161	26.692685
223.908078	6970.617137	26.697703
224.007621	6992.358526	26.702720
224.609005	6997.624237	26.707738
225.065340	7002.932742	26.712756
225.232408	7008.292869	26.717773
225.181907	7010.637973	26.722791
225.358237	7020.377632	26.727808
225.482613	7013.087806	26.732826
225.623109	7023.110139	26.737844
225.863613	7030.140000	26.742861
226.269434	7026.063521	26.747879
226.313745	7043.107038	26.752896
226.848861	7055.500122	26.757914
226.725027	7065.839221	26.762932
226.752293	7078.020581	26.767949
227.128052	7082.670015	26.772967
227.268948	7092.088051	26.777984
227.770099	7101.936497	26.783002
228.046170	7120.143063	26.788020
228.284788	7123.900082	26.793037
228.358689	7116.980977	26.798055
228.468373	7146.686782	26.803072
229.130050	7147.788499	26.808090
229.423779	7141.701423	26.813108
229.107087	7148.397636	26.818125
229.528414	7166.262440	26.823143
229.816992	7179.030116	26.828160
229.862079	7177.713852	26.833178
230.230035	7190.516881	26.838196
229.976385	7214.631317	26.843213
230.290273	7217.285030	26.848231
230.271727	7238.727724	26.853248
230.643012	7256.309487	26.858266
231.090585	7260.195319	26.863284
231.110755	7286.813196	26.868301
231.654777	7285.743139	26.873319
231.839659	7313.229436	26.878336
232.333352	7323.355398	26.883354
232.485038	7323.800375	26.888372
232.660470	7343.510376	26.893389
233.129303	7345.886052	26.898407
233.225579	7363.994898	26.903424
233.259068	7363.066804	26.908442
233.619337	7371.572726	26.913460
233.867648	7387.665880	26.918477
234.442544	7396.305200	26.923495
234.464983	7408.436456	26.928512
235.079760	7416.808988	26.933530
235.006966	7406.274000	26.938548
235.446965	7429.025565	26.943565
235.759915	7430.666802	26.948583
235.880771	7445.910092	26.953600
236.024524	7444.877863	26.958618
236.309361	7444.920002	26.963636
236.186450	7463.668596	26.968653
236.269626	7470.939340	26.973671
236.465313	7478.383356	26.978688
236.722662	7490.611784	26.983706
236.925070	7498.921054	26.988724
236.602619	7513.088645	26.993741
237.448023	7528.062301	26.998759
237.597285	7539.555774	27.003776
237.665808	7559.208353	27.008794
238.178631	7557.571214	27.013812
238.386176	7577.743794	27.018829
238.813244	7591.867521	27.023847
239.190483	7586.961390	27.028864
239.297622	7587.393019	27.033882
239.533724	7607.268380	27.038900
239.860631	7619.696702	27.043917
240.078243	7608.662053	27.048935
239.929507	7627.247764	27.053952
240.108636	7651.193202	27.058970
240.570780	7640.418555	27.063988
240.624122	7669.570212	27.069005
240.719223	7678.419945	27.074023
241.010571	7698.078891	27.079040
241.316474	7699.367986	27.084058
241.564861	7723.963459	27.089076
241.688811	7740.666175	27.094093
242.177214	7744.133316	27.099111
242.415792	7754.127919	27.104128
242.739924	7767.089510	27.109146
243.036416	7782.643497	27.114164
243.275041	7782.748085	27.119181
243.561917	7792.002449	27.124199
243.750868	7809.669013	27.129216
243.952859	7803.895300	27.134234
244.718459	7819.539790	27.139252
244.602634	7834.906973	27.144269
245.285050	7824.355174	27.149287
245.111720	7839.681169	27.154304
245.181043	7854.446024	27.159322
245.878105	7848.716917	27.164340
245.900585	7865.702694	27.169357
246.046246	7880.210692	27.174375
246.329285	7892.833509	27.179392
246.495999	7892.633242	27.184410
246.594657	7909.605352	27.189428
246.552182	7923.103931	27.194445
247.124946	7935.059765	27.199463
247.563700	7946.255611	27.204480
247.538448	7958.213937	27.209498
248.038957	7965.469547	27.214516
247.854251	7982.066720	27.219533
248.500645	7988.058194	27.224551
248.913826	7996.264115	27.229568
249.037805	8006.796490	27.234586
248.956208	8025.548253	27.239604
249.392972	8033.630043	27.244621
249.567224	8046.569344	27.249639
250.005100	8062.792749	27.254656
250.159987	8073.152641	27.259674
250.415761	8077.986761	27.264692
250.581018	8095.964323	27.269709
250.837525	8098.462101	27.274727
251.308932	8110.542035	27.279744
251.263367	8123.810733	27.284762
251.431761	8134.579264	27.289780
251.661332	8139.831479	27.294797
251.842982	8148.933661	27.299815
252.334448	8153.956072	27.304832
252.432836	8166.433081	27.309850
252.527103	8176.560348	27.314868
252.508285	8199.641965	27.319885
252.647529	8210.379787	27.324903
253.024730	8222.780927	27.329920
253.603650	8251.236177	27.334938
254.041950	8255.787885	27.339956
253.995196	8280.677618	27.344973
254.639749	8282.138623	27.349991
254.895824	8295.125687	27.355008
254.946273	8313.938600	27.360026
255.626515	8327.635920	27.365044
255.797902	8335.106273	27.370061
256.050724	8337.065267	27.375079
256.194463	8332.403067	27.380096
256.572861	8354.056751	27.385114
256.747094	8360.901873	27.390132
256.706033	8380.848413	27.395149
256.914920	8399.035781	27.400167
257.390664	8410.719464	27.405184
257.653755	8422.906826	27.410202
257.922557	8422.760708	27.415220
258.149071	8446.167538	27.420237
258.326521	8449.369657	27.425255
258.668277	8459.018187	27.430272
259.131071	8474.370519	27.435290
259.523469	8473.596823	27.440308
259.831224	8496.704354	27.445325
260.256914	8508.113989	27.450343
260.617952	8500.834505	27.455360
260.834055	8506.870780	27.460378
261.027099	8497.500928	27.465396
261.022049	8525.508007	27.470413
261.352879	8534.531957	27.475431
261.289425	8527.011264	27.480448
261.230529	8548.193153	27.485466
261.918669	8554.886024	27.490484
262.033470	8570.748752	27.495501
261.852772	8594.750307	27.500519
262.522271	8601.449318	27.505536
262.659367	8628.966121	27.510554
262.738688	8638.420133	27.515572
262.867632	8653.730256	27.520589
263.490796	8664.334222	27.525607
263.616954	8675.271585	27.530624
263.765443	8692.894497	27.535642
264.219492	8695.739000	27.540660
264.385288	8709.242862	27.545677
264.636033	8737.704532	27.550695
264.855388	8738.823381	27.555712
264.767005	8754.336646	27.560730
265.231267	8766.268742	27.565748
265.561116	8785.391824	27.570765
265.715697	8799.927624	27.575783
266.218762	8825.522259	27.580800
266.445254	8841.618105	27.585818
267.036529	8848.991887	27.590836
267.085818	8862.204020	27.595853
266.936579	8880.281838	27.600871
267.762115	8891.279825	27.605888
267.909735	8911.454713	27.610906
268.433892	8917.384609	27.615924
268.562815	8937.647500	27.620941
268.749274	8944.412250	27.625959
269.149168	8960.569901	27.630976
269.275838	8969.511767	27.635994
269.847602	8985.592080	27.641012
269.922195	8993.621169	27.646029
270.213141	9006.624149	27.651047
270.840671	9011.895084	27.656064
270.840256	9010.776742	27.661082
271.266484	9030.022881	27.666100
271.570310	9043.162733	27.671117
271.795752	9053.495928	27.676135
272.055877	9059.172475	27.681152
272.248493	9077.492713	27.686170
272.579316	9081.659690	27.691188
272.683641	9099.902351	27.696205
272.890891	9118.155385	27.701223
273.260509	9112.664504	27.706240
273.660146	9134.144386	27.711258
273.554926	9132.180264	27.716276
273.630145	9161.367543	27.721293
273.765080	9176.214924	27.726311
274.142608	9193.127126	27.731328
274.343097	9216.715978	27.736346
274.624827	9232.645267	27.741364
274.798686	9242.550459	27.746381
275.049712	9265.705995	27.751399
275.667311	9277.464545	27.756416
276.007069	9306.175158	27.761434
276.507548	9319.785977	27.766452
276.875692	9327.596903	27.771469
277.231059	9349.855746	27.776487
277.881167	9347.986434	27.781504
277.857361	9356.519305	27.786522
278.314253	9371.094433	27.791540
278.441876	9379.834935	27.796557
278.376649	9389.724033	27.801575
278.798140	9394.080860	27.806592
279.010502	9409.516176	27.811610
279.042471	9405.996397	27.816628
279.615679	9422.410225	27.821645
279.836051	9449.044900	27.826663
280.138429	9441.076687	27.831680
280.285352	9468.471490	27.836698
280.436689	9468.302774	27.841716
280.824348	9474.807482	27.846733
280.694337	9498.114609	27.851751
281.239646	9500.320281	27.856768
281.431721	9529.307473	27.861786
281.483873	9530.821327	27.866804
281.959578	9553.754597	27.871821
282.376185	9558.162223	27.876839
282.797671	9580.967247	27.881856
282.838586	9600.737084	27.886874
283.314108	9612.902579	27.891892
283.706510	9612.235071	27.896909
283.785714	9631.711607	27.901927
284.208723	9638.709684	27.906944
284.530787	9650.053297	27.911962
284.742155	9674.378122	27.916980
285.228474	9680.020035	27.921997
285.501821	9693.950703	27.927015
285.883646	9695.808264	27.932032
285.652001	9707.303916	27.937050
286.109674	9723.195062	27.942068
286.463755	9736.388898	27.947085
286.526134	9756.798467	27.952103
287.014608	9767.783155	27.957120
287.609354	9784.779057	27.962138
287.346601	9800.417990	27.967156
288.051174	9804.528752	27.972173
288.012718	9840.169698	27.977191
288.470382	9831.522954	27.982208
288.743354	9854.630653	27.987226
289.198654	9864.307643	27.992244
289.640991	9873.979231	27.997261
289.519491	9899.116898	28.002279
289.918836	9910.064744	28.007296
290.119734	9920.790821	28.012314
290.617417	9932.581596	28.017332
291.032777	9951.200684	28.022349
290.834671	9963.449434	28.027367
291.504546	9969.807074	28.032384
291.628001	9986.111022	28.037402
292.157816	10008.176989	28.042420
292.321254	9999.519201	28.047437
292.637460	10022.226780	28.052455
292.667307	10036.664434	28.057472
293.281815	10052.006807	28.062490
293.527940	10064.222612	28.067508
293.920785	10085.036798	28.072525
294.181112	10085.562136	28.077543
294.691908	10095.930452	28.082560
294.873738	10102.398200	28.087578
294.946964	10116.206516	28.092596
295.268189	10119.037449	28.097613
294.978461	10141.134678	28.102631
295.166922	10152.294171	28.107648
295.753212	10167.421198	28.112666
296.094420	10186.650899	28.117684
296.305303	10190.860130	28.122701
296.206024	10219.169096	28.127719
296.968829	10230.924541	28.132736
297.145016	10249.632094	28.137754
297.370640	10269.583891	28.142772
297.631208	10285.721898	28.147789
297.908928	10306.579137	28.152807
298.142684	10326.495480	28.157824
298.815073	10347.525578	28.162842
298.951610	10357.529535	28.167860
299.241417	10373.588212	28.172877
299.474737	10396.625546	28.177895
299.829621	10403.746989	28.182912
300.275119	10438.161236	28.187930
300.446092	10451.265263	28.192948
300.915758	10450.294614	28.197965
301.357000	10482.565070	28.202983
301.654584	10501.588457	28.208000
302.431026	10500.101040	28.213018
302.275448	10516.671182	28.218036
302.646922	10531.830454	28.223053
302.651970	10548.227074	28.228071
303.285788	10563.863990	28.233088
303.440853	10580.195812	28.238106
303.739188	10595.630846	28.243124
304.176837	10590.371778	28.248141
304.354341	10609.554527	28.253159
304.685559	10615.705922	28.258176
305.045138	10637.843628	28.263194
304.871636	10659.456788	28.268212
305.384099	10663.680656	28.273229
305.607472	10685.838173	28.278247
306.191047	10697.781530	28.283264
306.664806	10700.466673	28.288282
306.593790	10738.760868	28.293300
307.206655	10741.953509	28.298317
307.544921	10762.002321	28.303335
307.670962	10784.240031	28.308352
308.137192	10794.656074	28.313370
308.484492	10801.020625	28.318388
309.005593	10808.145284	28.323405
308.961789	10833.459042	28.328423
309.400649	10841.131997	28.333440
309.756212	10855.863634	28.338458
309.726225	10873.754053	28.343476
310.405757	10879.140545	28.348493
310.519142	10905.818465	28.353511
310.865717	10905.922019	28.358528
311.157185	10919.504649	28.363546
311.046838	10932.630714	28.368564
311.722067	10939.634462	28.373581
311.961296	10958.668909	28.378599
312.437813	10965.805865	28.383616
312.947981	10977.236200	28.388634
313.026027	10989.899818	28.393652
313.450378	10999.922870	28.398669
313.654228	11009.918107	28.403687
313.957626	11018.947543	28.408704
314.365821	11038.712284	28.413722
314.346473	11052.767205	28.418740
314.849503	11045.542187	28.423757
315.063883	11070.296935	28.428775
315.301745	11076.671175	28.433792
315.527305	11084.486861	28.438810
315.545690	11111.388848	28.443828
316.125784	11131.130644	28.448845
316.047528	11150.907341	28.453863
316.273820	11171.129394	28.458880
316.889727	11189.436300	28.463898
317.163986	11215.602740	28.468916
317.617342	11234.521951	28.473933
317.622523	11264.231325	28.478951
317.992436	11278.140205	28.483968
318.364270	11307.565743	28.488986
318.692270	11330.930993	28.494004
319.284200	11353.646225	28.499021
319.677720	11364.960468	28.504039
319.814121	11387.491377	28.509056
320.196079	11405.270731	28.514074
320.457045	11428.249356	28.519092
321.117320	11439.557741	28.524109
321.577214	11465.791050	28.529127
321.724258	11490.624511	28.534144
322.187796	11485.542430	28.539162
322.535971	11515.207865	28.544180
322.919823	11515.389701	28.549197
323.231788	11544.640285	28.554215
323.589198	11549.262183	28.559232
323.974640	11556.866889	28.564250
324.140213	11573.288230	28.569268
324.631840	11578.484551	28.574285
324.428981	11605.229059	28.579303
324.712809	11604.637417	28.584320
325.200986	11623.663724	28.589338
325.303830	11647.907700	28.594356
326.069061	11664.848860	28.599373
326.560048	11674.711809	28.604391
326.640901	11690.508077	28.609408
327.056813	11708.471273	28.614426
327.635713	11727.646373	28.619444
327.884429	11723.753271	28.624461
328.217379	11743.341837	28.629479
328.307716	11755.825475	28.634496
329.037635	11762.414576	28.639514
329.134961	11792.567194	28.644532
329.383835	11787.209119	28.649549
329.580766	11792.985128	28.654567
329.907084	11811.572901	28.659584
330.053498	11809.120481	28.664602
330.349279	11838.350010	28.669620
330.674916	11845.686361	28.674637
330.858677	11866.504460	28.679655
330.987171	11887.521473	28.684672
331.860086	11905.983097	28.689690
331.710022	11920.291841	28.694708
332.174673	11944.289144	28.699725
332.163873	11956.446293	28.704743
332.375694	11986.353585	28.709760
332.795481	12009.530528	28.714778
333.334719	12038.468009	28.719796
333.717272	12051.722313	28.724813
334.142703	12074.955914	28.729831
334.267837	12098.610878	28.734848
334.949444	12105.963827	28.739866
335.106601	12132.701673	28.744884
335.775021	12157.584191	28.749901
336.245427	12166.742366	28.754919
336.599119	12178.281199	28.759936
337.350280	12192.071333	28.764954
337.310757	12205.975482	28.769972
337.628967	12223.363167	28.774989
338.225902	12234.942186	28.780007
338.114834	12256.500840	28.785024
338.823409	12257.425315	28.790042
338.634697	12276.219113	28.795060
339.000014	12282.440142	28.800077
339.529809	12312.210038	28.805095
339.483387	12318.136404	28.810112
340.033025	12338.731555	28.815130
340.173092	12366.800568	28.820148
340.340438	12386.710537	28.825165
341.051428	12411.025684	28.830183
340.998369	12436.836320	28.835200
341.628736	12451.845684	28.840218
342.093868	12477.628120	28.845236
342.556438	12488.865105	28.850253
343.128375	12506.411033	28.855271
343.428144	12522.274425	28.860288
343.746484	12534.573410	28.865306
343.809657	12561.202823	28.870324
344.358188	12560.158095	28.875341
344.629423	12581.169655	28.880359
344.684653	12602.633623	28.885376
345.312231	12615.753151	28.890394
345.621790	12630.305737	28.895412
345.837479	12658.073973	28.900429
345.989261	12672.090530	28.905447
346.193850	12700.705187	28.910464
346.766181	12712.763914	28.915482
346.987632	12737.948258	28.920500
347.527009	12764.310084	28.925517
348.141569	12762.772318	28.930535
347.930486	12790.868556	28.935552
348.560645	12802.558032	28.940570
348.950963	12816.405063	28.945588
348.961760	12840.073107	28.950605
349.961675	12853.064045	28.955623
349.827655	12876.208368	28.960640
350.273488	12899.330377	28.965658
350.354979	12909.270612	28.970676
350.563024	12931.431305	28.975693
351.063924	12942.390766	28.980711
351.181916	12973.208346	28.985728
351.829338	12991.944166	28.990746
352.050687	13024.670310	28.995764
352.323076	13046.416528	29.000781
352.976160	13062.724800	29.005799
353.216677	13087.301773	29.010816
353.982533	13099.864043	29.015834
354.255589	13124.292435	29.020852
354.508532	13143.561620	29.025869
355.307810	13139.902170	29.030887
354.967918	13182.516000	29.035904
355.623089	13183.396315	29.040922
355.650619	13212.431950	29.045940
356.135942	13238.421057	29.050957
356.617482	13251.712297	29.055975
356.925771	13285.435446	29.060992
357.502242	13294.980722	29.066010
358.044675	13320.466146	29.071028
357.870730	13337.735570	29.076045
358.510188	13355.072378	29.081063
358.737984	13382.964477	29.086080
359.155409	13393.882172	29.091098
359.530752	13410.805667	29.096116
360.018696	13437.761222	29.101133
360.378846	13451.904102	29.106151
360.456598	13466.289474	29.111168
361.033946	13488.048044	29.116186
361.241690	13509.464191	29.121204
361.510072	13533.626056	29.126221
361.918671	13560.385088	29.131239
362.241001	13582.685361	29.136256
362.544404	13601.713299	29.141274
363.008898	13616.291733	29.146292
362.960647	13642.181991	29.151309
363.661880	13658.122910	29.156327
364.141961	13685.958536	29.161344
364.494804	13696.442484	29.166362
364.959984	13725.968146	29.171380
365.037966	13751.070861	29.176397
365.692334	13776.593135	29.181415
365.971910	13794.868738	29.186432
366.144494	13809.355824	29.191450
366.802638	13837.767214	29.196468
366.918937	13853.972070	29.201485
367.223122	13866.916630	29.206503
367.525375	13906.138475	29.211520
368.051161	13913.901390	29.216538
368.302570	13928.165556	29.221556
368.348182	13955.617295	29.226573
368.858707	13974.218809	29.231591
369.214673	13997.197012	29.236608
369.845335	14029.177502	29.241626
370.394789	14046.563490	29.246644
370.780252	14064.181676	29.251661
371.230642	14092.802586	29.256679
371.809076	14103.157684	29.261696
372.009419	14103.862575	29.266714
372.683250	14123.300811	29.271732
372.530057	14147.197451	29.276749
373.038970	14147.374464	29.281767
373.375010	14174.753948	29.286784
373.655181	14197.070300	29.291802
374.285791	14220.560343	29.296820
374.505980	14242.817244	29.301837
374.708790	14259.454495	29.306855
374.895166	14282.557962	29.311872
375.201788	14305.358123	29.316890
375.596637	14339.501196	29.321908
375.935091	14364.463143	29.326925
376.686737	14386.471141	29.331943
377.237366	14404.580792	29.336960
377.335073	14439.137683	29.341978
377.839971	14447.885847	29.346996
378.183553	14471.230797	29.352013
378.712363	14489.225944	29.357031
379.024819	14519.178464	29.362048
379.392654	14541.424081	29.367066
379.657583	14561.046214	29.372084
379.648060	14586.012704	29.377101
380.189324	14619.560572	29.382119
380.662462	14637.118119	29.387136
380.790983	14663.092318	29.392154
381.467846	14679.235885	29.397172
381.824324	14700.263356	29.402189
382.048128	14723.210575	29.407207
382.168048	14757.302152	29.412224
382.940769	14784.305538	29.417242
383.764083	14812.091482	29.422260
383.767358	14831.188655	29.427277
384.383757	14851.705240	29.432295
384.949375	14868.049273	29.437312
385.012384	14883.903654	29.442330
385.346779	14907.679994	29.447348
385.671818	14934.571656	29.452365
386.286895	14953.418281	29.457383
386.404711	14988.246670	29.462400
386.645233	15003.082254	29.467418
387.419621	15020.228440	29.472436
387.814125	15040.205462	29.477453
388.164646	15046.933332	29.482471
388.399411	15075.413803	29.487488
388.741159	15088.062433	29.492506
389.345642	15114.378793	29.497524
389.437790	15131.564832	29.502541
390.094873	15158.081308	29.507559
390.037364	15180.780690	29.512576
390.862206	15189.112728	29.517594
391.118584	15209.437505	29.522612
390.993796	15239.430795	29.527629
391.447503	15266.824384	29.532647
392.113873	15286.661184	29.537664
391.981361	15311.149137	29.542682
392.641032	15338.682150	29.547700
393.257658	15366.295186	29.552717
393.707089	15401.408617	29.557735
394.204933	15429.546408	29.562752
394.323157	15444.103339	29.567770
394.789403	15474.640492	29.572788
395.168826	15495.378543	29.577805
395.653395	15525.200900	29.582823
396.170139	15550.526363	29.587840
395.987041	15585.277598	29.592858
396.978506	15611.629592	29.597876
397.269201	15635.291409	29.602893
397.880420	15660.067937	29.607911
398.191151	15684.104328	29.612928
398.619077	15716.183441	29.617946
399.368694	15725.489807	29.622964
399.287940	15761.278304	29.627981
399.650779	15781.349316	29.632999
400.419564	15789.896688	29.638016
400.584438	15825.970555	29.643034
401.288413	15839.301737	29.648052
401.532801	15864.303948	29.653069
402.122523	15887.265066	29.658087
402.612437	15906.571819	29.663104
402.601454	15926.377831	29.668122
403.294086	15938.473891	29.673140
403.639836	15977.079928	29.678157
403.875328	15999.586708	29.683175
404.325568	16018.782815	29.688192
404.505859	16048.717851	29.693210
405.008311	16058.875893	29.698228
405.314851	16090.517418	29.703245
405.778708	16108.757469	29.708263
406.318858	16130.644325	29.713280
406.600455	16169.353180	29.718298
407.190264	16187.302033	29.723316
407.388109	16221.377945	29.728333
407.966170	16230.087828	29.733351
408.414928	16257.696546	29.738368
408.440107	16282.948313	29.743386
408.990885	16299.812517	29.748404
409.429283	16328.372300	29.753421
410.014500	16350.840011	29.758439
410.436328	16360.257256	29.763456
410.100578	16387.788474	29.768474
410.736129	16412.672959	29.773492
411.294438	16434.123156	29.778509
411.433943	16471.779357	29.783527
412.035617	16490.225042	29.788544
412.116652	16513.212248	29.793562
412.799798	16544.674833	29.798580
412.914947	16572.523667	29.803597
413.519080	16600.776871	29.808615
414.029419	16623.625966	29.813632
414.464184	16662.635439	29.818650
415.267253	16680.838460	29.823668
415.561469	16707.835863	29.828685
415.995478	16732.017029	29.833703
416.385393	16751.708064	29.838720
416.958982	16773.401551	29.843738
417.099738	16796.881191	29.848756
417.564976	16836.452335	29.853773
418.051601	16849.769036	29.858791
418.794852	16865.206671	29.863808
418.592433	16902.143077	29.868826
419.114302	16914.929463	29.873844
419.839684	16946.385551	29.878861
420.151147	16979.230965	29.883879
420.848389	17002.927543	29.888896
421.107120	17023.468892	29.893914
421.604799	17039.728837	29.898932
421.815242	17073.194829	29.903949
422.185928	17087.623627	29.908967
422.863595	17118.864655	29.913984
423.017980	17152.439939	29.919002
423.546380	17178.718424	29.924020
423.971255	17203.257862	29.929037
423.877927	17233.491135	29.934055
424.703502	17264.402810	29.939072
425.040063	17302.272535	29.944090
425.664119	17317.640450	29.949108
426.112048	17355.208130	29.954125
426.617943	17371.343698	29.959143
427.274691	17390.056674	29.964160
427.740268	17424.255566	29.969178
428.308034	17429.031577	29.974196
428.824626	17453.562705	29.979213
429.039954	17472.268949	29.984231
429.554580	17477.652623	29.989248
429.834984	17517.021902	29.994266
430.495229	17519.395924	29.999284
430.742131	17554.202357	30.004301
431.096696	17572.195232	30.009319
431.488406	17595.384734	30.014336
431.640928	17623.194073	30.019354
431.924882	17638.749954	30.024372
432.708496	17659.547289	30.029389
432.969122	17694.467987	30.034407
433.112966	17709.609665	30.039424
434.059175	17736.114846	30.044442
433.970838	17756.318581	30.049460
434.273009	17782.397729	30.054477
434.499646	17815.952113	30.059495
435.105195	17836.069809	30.064512
434.896152	17873.171977	30.069530
435.526640	17910.835342	30.074548
435.704999	17946.228758	30.079565
436.391953	17984.413216	30.084583
436.879559	18018.484323	30.089600
437.303797	18058.813540	30.094618
437.805657	18092.195540	30.099636
438.451090	18110.926549	30.104653
438.799447	18165.408926	30.109671
439.651220	18183.826442	30.114688
439.942320	18213.174986	30.119706
440.583577	18256.693750	30.124724
441.198341	18270.270400	30.129741
441.552262	18313.875260	30.134759
442.476189	18332.431459	30.139776
442.564517	18359.157458	30.144794
442.699529	18386.467408	30.149812
443.671674	18403.297497	30.154829
443.825779	18429.962350	30.159847
444.386005	18443.811231	30.164864
444.752271	18485.940182	30.169882
445.291158	18501.386629	30.174900
445.856662	18535.530322	30.179917
445.916795	18568.090007	30.184935
446.649689	18584.710375	30.189952
446.645412	18617.719410	30.194970
447.350269	18648.543048	30.199988
447.932689	18665.679220	30.205005
447.953123	18707.973715	30.210023
448.791557	18740.545988	30.215040
449.004744	18772.387995	30.220058
449.434104	18806.249632	30.225076
449.847989	18826.670423	30.230093
449.967959	18870.635780	30.235111
450.753032	18905.378399	30.240128
451.081160	18933.999541	30.245146
451.430484	18962.480739	30.250164
452.151540	18997.084937	30.255181
452.426376	19035.135266	30.260199
453.058636	19057.951215	30.265216
453.293186	19102.936819	30.270234
454.156611	19129.670584	30.275252
454.842269	19160.134498	30.280269
454.799292	19192.754435	30.285287
455.114062	19219.497018	30.290304
455.628998	19257.772254	30.295322
456.315572	19277.023745	30.300340
456.654658	19297.672833	30.305357
456.694193	19327.019457	30.310375
457.642910	19356.142548	30.315392
458.270109	19381.748159	30.320410
458.573327	19413.710213	30.325428
459.228654	19431.137608	30.330445
459.405540	19465.129095	30.335463
459.644769	19483.367776	30.340480
460.234845	19523.422777	30.345498
461.059444	19548.795231	30.350516
461.178837	19562.909848	30.355533
461.248517	19598.237710	30.360551
461.834461	19628.577077	30.365568
462.304623	19664.634663	30.370586
462.611303	19690.136712	30.375604
463.750696	19728.039581	30.380621
463.952619	19756.082282	30.385639
463.960377	19792.996581	30.390656
464.826475	19831.778361	30.395674
465.246380	19855.453409	30.400692
465.906517	19885.322748	30.405709
466.068145	19924.000822	30.410727
466.730535	19963.990703	30.415744
467.270617	19992.527260	30.420762
467.553219	20029.932249	30.425780
468.112840	20052.235580	30.430797
468.244403	20093.426625	30.435815
468.563309	20125.023813	30.440832
469.256099	20162.019242	30.445850
469.772055	20195.149935	30.450868
470.613718	20234.118126	30.455885
470.980108	20272.492358	30.460903
471.564239	20298.269745	30.465920
471.951423	20334.658278	30.470938
472.318203	20363.838557	30.475956
473.087293	20391.032887	30.480973
473.318598	20432.386516	30.485991
474.104039	20458.183285	30.491008
474.595309	20491.849322	30.496026
475.434853	20520.549404	30.501044
475.505558	20543.269167	30.506061
475.683108	20577.522450	30.511079
476.331346	20593.525692	30.516096
476.876551	20631.580543	30.521114
477.109915	20667.367882	30.526132
477.754145	20696.834554	30.531149
478.000278	20739.106062	30.536167
478.767292	20769.496766	30.541184
479.192895	20798.140053	30.546202
479.800354	20837.827877	30.551220
480.274794	20861.357943	30.556237
480.452466	20900.358362	30.561255
481.133066	20923.944672	30.566272
481.691791	20950.157175	30.571290
481.765072	20988.660182	30.576308
482.727670	21009.335848	30.581325
483.152252	21030.935192	30.586343
483.737296	21056.644381	30.591360
484.198865	21077.559037	30.596378
484.137240	21105.216531	30.601396
485.263151	21126.938973	30.606413
485.432692	21154.900737	30.611431
485.872796	21175.136928	30.616448
486.793191	21199.532068	30.621466
487.095593	21227.917761	30.626484
487.410768	21245.561643	30.631501
487.794427	21284.908227	30.636519
488.308324	21312.663418	30.641536
488.816064	21339.910878	30.646554
489.347334	21369.642529	30.651572
489.752107	21390.538298	30.656589
489.904590	21434.512756	30.661607
490.463583	21460.379545	30.666624
491.109982	21492.814113	30.671642
491.398883	21535.521985	30.676660
491.629267	21572.175817	30.681677
492.257795	21600.945757	30.686695
492.672842	21635.811682	30.691712
492.951328	21682.003457	30.696730
493.563232	21724.899811	30.701748
494.070025	21754.845584	30.706765
494.670044	21804.686531	30.711783
495.316722	21839.191525	30.716800
495.881537	21875.954244	30.721818
496.645115	21915.407276	30.726836
496.868169	21944.732314	30.731853
497.657969	21983.829290	30.736871
498.022271	22016.880089	30.741888
498.516038	22056.746622	30.746906
499.045156	22098.412787	30.751924
499.329441	22126.000429	30.756941
499.655304	22176.705322	30.761959
500.279172	22212.596214	30.766976
501.034881	22239.408783	30.771994
501.275702	22291.033330	30.777012
501.411671	22323.149241	30.782029
502.253902	22364.041635	30.787047
503.009641	22403.129326	30.792064
504.098126	22432.603314	30.797082
504.327314	22464.958275	30.802100
505.023580	22477.305220	30.807117
505.121603	22516.482996	30.812135
505.626229	22557.163457	30.817152
506.191321	22592.347845	30.822170
506.933327	22628.906094	30.827188
507.353681	22649.654556	30.832205
507.842598	22683.395760	30.837223
508.507034	22720.623454	30.842240
508.721679	22744.268609	30.847258
509.421695	22782.957341	30.852276
509.916616	22796.541680	30.857293
510.516517	22831.914815	30.862311
510.628190	22860.262154	30.867328
511.247770	22885.508858	30.872346
511.720986	22909.844784	30.877364
511.932147	22940.007666	30.882381
512.589616	22970.601238	30.887399
513.393506	22997.112061	30.892416
513.986954	23027.525333	30.897434
513.940163	23067.139474	30.902452
514.545894	23092.478506	30.907469
514.984280	23124.085525	30.912487
515.233252	23164.634990	30.917504
515.917818	23208.331928	30.922522
515.986249	23251.761659	30.927540
516.602094	23297.471996	30.932557
517.019590	23343.517307	30.937575
517.759110	23377.785610	30.942592
518.167886	23425.975762	30.947610
518.499072	23466.233282	30.952628
519.344031	23503.166260	30.957645
519.989178	23543.875709	30.962663
520.563520	23586.060813	30.967680
521.614857	23617.912242	30.972698
521.933672	23658.472322	30.977716
522.183469	23701.486072	30.982733
522.895588	23735.484616	30.987751
523.144166	23775.426831	30.992768
523.901195	23807.829635	30.997786
524.146457	23865.103099	31.002804
524.914029	23899.998209	31.007821
525.543367	23930.253112	31.012839
525.863637	23989.542575	31.017856
526.732442	24012.567127	31.022874
527.306995	24049.559416	31.027892
527.467773	24084.737479	31.032909
528.392974	24123.225840	31.037927
528.796163	24155.326527	31.042944
529.363135	24191.514543	31.047962
529.640743	24237.939978	31.052980
530.372674	24275.207839	31.057997
531.087203	24310.549475	31.063015
531.277194	24345.769149	31.068032
532.418839	24382.430849	31.073050
532.755769	24421.427967	31.078068
533.043754	24455.834327	31.083085
533.634703	24486.484747	31.088103
534.137507	24537.487236	31.093120
534.598384	24568.346008	31.098138
534.879761	24618.923213	31.103156
535.472380	24647.056918	31.108173
536.549167	24684.834818	31.113191
537.210848	24725.239814	31.118208
537.830915	24743.795335	31.123226
538.162379	24756.642517	31.128244
538.765743	24794.360596	31.133261
539.368535	24815.720896	31.138279
539.301073	24852.192644	31.143296
540.285662	24867.280957	31.148314
540.852417	24912.490160	31.153332
541.092593	24935.687078	31.158349
541.772721	24971.558719	31.163367
541.733207	25002.600439	31.168384
542.511152	25034.246188	31.173402
542.566463	25081.587026	31.178420
543.122658	25116.970641	31.183437
543.693536	25158.415263	31.188455
543.995672	25213.260619	31.193472
544.673679	25238.833409	31.198490
545.318731	25284.811066	31.203508
545.943680	25342.792689	31.208525
546.911632	25374.552223	31.213543
547.451623	25412.365359	31.218560
547.910816	25450.772032	31.223578
548.358434	25503.027116	31.228596
548.685943	25532.984952	31.233613
549.456449	25574.736809	31.238631
550.221320	25616.420350	31.243648
550.683791	25641.260830	31.248666
551.260428	25698.645645	31.253684
551.351677	25743.231029	31.258701
552.221945	25777.841333	31.263719
552.564352	25827.085238	31.268736
553.303085	25870.249110	31.273754
553.813847	25925.316552	31.278772
554.196555	25965.192463	31.283789
554.909638	26002.931371	31.288807
555.407370	26062.982533	31.293824
556.182157	26095.851177	31.298842
556.594251	26147.826477	31.303860
557.429727	26194.594149	31.308877
557.738002	26225.423706	31.313895
558.291275	26281.337996	31.318912
558.904380	26311.830046	31.323930
559.576572	26368.489079	31.328948
559.640176	26404.513337	31.333965
560.345088	26457.140209	31.338983
560.802408	26503.382093	31.344000
561.636063	26545.566023	31.349018
561.961229	26597.588924	31.354036
562.259638	26637.230979	31.359053
563.266475	26693.956822	31.364071
563.397565	26745.886636	31.369088
564.316915	26793.643230	31.374106
565.211541	26830.869874	31.379124
565.997074	26878.318721	31.384141
566.487464	26921.257113	31.389159
566.841261	26954.534912	31.394176
567.803333	26999.140287	31.399194
568.174859	27020.333171	31.404212
568.640276	27071.582883	31.409229
569.274646	27092.086396	31.414247
569.643502	27134.561769	31.419264
570.236625	27169.566660	31.424282
570.784435	27212.920545	31.429300
571.197344	27252.660117	31.434317
571.621112	27290.719940	31.439335
571.883939	27337.539600	31.444352
572.686079	27372.197290	31.449370
572.991064	27437.611741	31.454388
573.524652	27495.147700	31.459405
574.590209	27518.432772	31.464423
575.133381	27582.382272	31.469440
575.752625	27624.623667	31.474458
576.699279	27663.151022	31.479476
577.100594	27708.180152	31.484493
577.606109	27746.732268	31.489511
578.227987	27803.464242	31.494528
578.951839	27834.942933	31.499546
579.437926	27873.400749	31.504564
579.841617	27933.306831	31.509581
580.473541	27968.681522	31.514599
580.940200	28005.811227	31.519616
581.436207	28053.870621	31.524634
581.966369	28114.192143	31.529652
582.375467	28144.993558	31.534669
583.310609	28183.806057	31.539687
583.906119	28241.144141	31.544704
584.391747	28291.405697	31.549722
585.016156	28340.663583	31.554740
585.401171	28378.424859	31.559757
586.197595	28424.338539	31.564775
586.908115	28477.316217	31.569792
587.182902	28528.225077	31.574810
587.933626	28568.306463	31.579828
588.439346	28618.926698	31.584845
589.238553	28671.731729	31.589863
589.356152	28735.536096	31.594880
590.280765	28776.839946	31.599898
590.941455	28826.567860	31.604916
591.453587	28884.726756	31.609933
592.312812	28919.257339	31.614951
592.588478	28977.469985	31.619968
593.219896	29027.252027	31.624986
593.771481	29071.197304	31.630004
594.433400	29119.091605	31.635021
595.443047	29168.262290	31.640039
595.510888	29236.066672	31.645056
595.935607	29276.507450	31.650074
596.682070	29328.049698	31.655092
596.996505	29384.169563	31.660109
598.067704	29431.213231	31.665127
598.446660	29480.680713	31.670144
598.962465	29545.633563	31.675162
599.757955	29578.320847	31.680180
600.314348	29638.418499	31.685197
601.089714	29664.676236	31.690215
601.121872	29712.683608	31.695232
602.149003	29762.532535	31.700250
602.985831	29807.717190	31.705268
603.437525	29859.033849	31.710285
603.868475	29896.231877	31.715303
604.580818	29937.985387	31.720320
605.144823	29986.583377	31.725338
605.787029	30031.197630	31.730356
606.027206	30076.747539	31.735373
606.881203	30125.507789	31.740391
607.461136	30177.072942	31.745408
607.864506	30240.074915	31.750426
608.373155	30277.765754	31.755444
608.755217	30349.663264	31.760461
609.578780	30394.084149	31.765479
610.080008	30449.185051	31.770496
610.575182	30523.312693	31.775514
611.384505	30573.321716	31.780532
612.328912	30627.975978	31.785549
613.032405	30665.975529	31.790567
613.500494	30724.521522	31.795584
614.034868	30782.371593	31.800602
615.112289	30828.828875	31.805620
615.597919	30876.816306	31.810637
616.521729	30928.251843	31.815655
617.327092	30973.236700	31.820672
618.097227	31012.504626	31.825690
618.768720	31059.635566	31.830708
618.951895	31102.940487	31.835725
619.821940	31136.139130	31.840743
620.408469	31180.267350	31.845760
620.752446	31231.126343	31.850778
621.546532	31267.382333	31.855796
621.956255	31317.137322	31.860813
622.636225	31368.696607	31.865831
623.412406	31418.552733	31.870848
624.104491	31465.312755	31.875866
624.993547	31506.701699	31.880884
625.578715	31557.854279	31.885901
626.272359	31592.420058	31.890919
626.919940	31640.139638	31.895936
627.125687	31693.594300	31.900954
627.761069	31729.019175	31.905972
628.202028	31781.966983	31.910989
628.774815	31829.736852	31.916007
629.470475	31879.745903	31.921024
629.672560	31927.674383	31.926042
630.526272	31978.342613	31.931060
630.795111	32040.884321	31.936077
631.533136	32094.449392	31.941095
632.120785	32151.742575	31.946112
632.760144	32205.810756	31.951130
633.626533	32263.163968	31.956148
633.808149	32312.562672	31.961165
634.703512	32355.582527	31.966183
635.360522	32402.629788	31.971200
635.928549	32449.043536	31.976218
636.394099	32501.721790	31.981236
637.118344	32570.059606	31.986253
637.613719	32609.573710	31.991271
638.012482	32674.787725	31.996288
638.572114	32727.782724	32.001306
639.568992	32793.149431	32.006324
640.019262	32840.675359	32.011341
640.392742	32902.338318	32.016359
641.226858	32958.181171	32.021376
641.892077	33016.242094	32.026394
643.378707	33061.280241	32.031412
643.904612	33135.856117	32.036429
644.201508	33184.261789	32.041447
645.053257	33231.899879	32.046464
645.481651	33295.361964	32.051482
646.036724	33346.695128	32.056500
646.796990	33408.574234	32.061517
647.639599	33463.930373	32.066535
648.447384	33512.941343	32.071552
648.736894	33566.398186	32.076570
649.591806	33626.532257	32.081588
650.089926	33676.743725	32.086605
650.604482	33734.077682	32.091623
651.433493	33801.453387	32.096640
651.928581	33853.808098	32.101658
652.921441	33914.340553	32.106676
653.516776	33962.611127	32.111693
654.397495	34019.411711	32.116711
655.199736	34080.585171	32.121728
655.861939	34134.711199	32.126746
656.392023	34172.248338	32.131764
657.177367	34231.946422	32.136781
657.804193	34284.264175	32.141799
658.397255	34324.928608	32.146816
658.798073	34388.369314	32.151834
659.831969	34436.078028	32.156852
660.371513	34486.405156	32.161869
660.927240	34550.400349	32.166887
661.658402	34603.553748	32.171904
662.107592	34654.073903	32.176922
662.943140	34705.505338	32.181940
663.684294	34771.866424	32.186957
664.481686	34823.234936	32.191975
665.226886	34861.308469	32.196992
665.933175	34920.160886	32.202010
666.809795	34953.744527	32.207028
667.180141	35017.823057	32.212045
667.881493	35064.464103	32.217063
668.345580	35126.937494	32.222080
668.736300	35174.933609	32.227098
669.621509	35212.779139	32.232116
670.297255	35273.601934	32.237133
670.854569	35318.017011	32.242151
671.364928	35362.135423	32.247168
671.787442	35429.724336	32.252186
672.529206	35475.534023	32.257204
673.012102	35526.782944	32.262221
673.796602	35579.297218	32.267239
674.450274	35634.183045	32.272256
675.012782	35692.930234	32.277274
675.892524	35748.980161	32.282292
676.379335	35800.476810	32.287309
676.792068	35870.594635	32.292327
677.978568	35921.365409	32.297344
678.008053	35988.264002	32.302362
678.744624	36051.853062	32.307380
679.840527	36110.573546	32.312397
680.614976	36187.007487	32.317415
681.283979	36234.733736	32.322432
681.859441	36293.611825	32.327450
682.942016	36352.857123	32.332468
683.634133	36421.018819	32.337485
683.959104	36472.620555	32.342503
684.824780	36537.761175	32.347520
685.714635	36588.450352	32.352538
686.408182	36661.859680	32.357556
687.241401	36701.053817	32.362573
687.643972	36757.060121	32.367591
688.483457	36817.572364	32.372608
689.157806	36867.118970	32.377626
689.879981	36926.751615	32.382644
690.289274	36986.137883	32.387661
690.847527	37047.748917	32.392679
691.826275	37099.336778	32.397696
692.353800	37184.107673	32.402714
692.984506	37245.605415	32.407732
694.184738	37293.051440	32.412749
694.965299	37360.364088	32.417767
695.744947	37408.121784	32.422784
696.080878	37467.809960	32.427802
697.097078	37521.854337	32.432820
697.704523	37581.669969	32.437837
698.483948	37634.721257	32.442855
699.235344	37684.660061	32.447872
699.916948	37739.321287	32.452890
700.958350	37803.279966	32.457908
701.480476	37856.866427	32.462925
702.047077	37909.602437	32.467943
702.533522	37972.902754	32.472960
703.036039	38025.408091	32.477978
704.006141	38081.616983	32.482996
704.662733	38132.322729	32.488013
704.769925	38181.307581	32.493031
705.798643	38248.527504	32.498048
706.385521	38322.322127	32.503066
707.205624	38364.341460	32.508084
708.055114	38425.914317	32.513101
708.718371	38469.020040	32.518119
709.491650	38535.184346	32.523136
709.920398	38572.589809	32.528154
710.600054	38638.917643	32.533172
711.193786	38678.952370	32.538189
711.756546	38751.131771	32.543207
712.695636	38797.750076	32.548224
713.409418	38861.684509	32.553242
714.117846	38916.485609	32.558260
714.785008	38985.760684	32.563277
715.383471	39044.534345	32.568295
716.285104	39102.354849	32.573312
717.281743	39177.660053	32.578330
717.449943	39229.112262	32.583348
717.911430	39293.356551	32.588365
718.479213	39356.740547	32.593383
719.517018	39421.456502	32.598400
720.368277	39481.711516	32.603418
720.779590	39566.539656	32.608436
721.697461	39634.322018	32.613453
722.415803	39713.608197	32.618471
723.530491	39764.167056	32.623488
723.978286	39849.191061	32.628506
724.973189	39903.809398	32.633524
725.960402	39970.090317	32.638541
726.143454	40034.798034	32.643559
726.928051	40101.234719	32.648576
728.173033	40159.008891	32.653594
728.818389	40225.703190	32.658612
729.417268	40287.647548	32.663629
729.923552	40343.242358	32.668647
730.900253	40407.024055	32.673664
731.624945	40481.703398	32.678682
732.487203	40546.369580	32.683700
733.282967	40605.807932	32.688717
733.848708	40671.165191	32.693735
734.680140	40729.566960	32.698752
735.765764	40793.517269	32.703770
735.932737	40861.660602	32.708788
737.055852	40916.887842	32.713805
737.960717	40983.608446	32.718823
738.266218	41055.080033	32.723840
738.788548	41117.228826	32.728858
739.556878	41186.252308	32.733876
740.391665	41244.560682	32.738893
740.759361	41321.637667	32.743911
741.845412	41383.789154	32.748928
742.706144	41458.271323	32.753946
743.445032	41525.105621	32.758964
744.019995	41595.050986	32.763981
744.654314	41661.341031	32.768999
745.640434	41728.285006	32.774016
746.255300	41803.110609	32.779034
746.968894	41852.839009	32.784052
747.744540	41914.552943	32.789069
748.450903	41980.179839	32.794087
749.194776	42038.281440	32.799104
750.001521	42098.502311	32.804122
750.516832	42166.434506	32.809140
751.220181	42226.792146	32.814157
752.005939	42299.110335	32.819175
752.595919	42356.225001	32.824192
752.895817	42430.084652	32.829210
753.379877	42508.406981	32.834228
754.652980	42572.047047	32.839245
755.224042	42664.007966	32.844263
755.853496	42737.759696	32.849280
756.795304	42805.418333	32.854298
757.676577	42890.848946	32.859316
758.703271	42968.585445	32.864333
759.611686	43038.180776	32.869351
760.231807	43115.632524	32.874368
760.820035	43188.405420	32.879386
761.459243	43257.284280	32.884404
762.532837	43336.737277	32.889421
763.303994	43405.403303	32.894439
763.893594	43472.423492	32.899456
764.714489	43552.646385	32.904474
765.153849	43633.438253	32.909492
766.576396	43702.582192	32.914509
767.326787	43782.410444	32.919527
768.293587	43851.166968	32.924544
768.828371	43924.232218	32.929562
769.462460	43992.919239	32.934580
770.703691	44058.869527	32.939597
771.216118	44135.623743	32.944615
771.770150	44209.747065	32.949632
772.944340	44288.551195	32.954650
773.322332	44362.517070	32.959668
774.318261	44434.671939	32.964685
775.026904	44505.093624	32.969703
775.668009	44589.706482	32.974720
776.713363	44659.740804	32.979738
777.035764	44739.669977	32.984756
778.150694	44810.327921	32.989773
778.976758	44895.811912	32.994791
779.669880	44958.969471	32.999808
780.308412	45038.272380	33.004826
781.704126	45115.663230	33.009844
782.100858	45191.484633	33.014861
782.644590	45275.128881	33.019879
783.753203	45335.092135	33.024896
784.329683	45418.444772	33.029914
784.959485	45502.382424	33.034932
786.017902	45574.935891	33.039949
786.908541	45652.665064	33.044967
787.732149	45728.398765	33.049984
788.633543	45792.933259	33.055002
789.187545	45872.158765	33.060020
790.181954	45909.824574	33.065037
790.924501	45993.131435	33.070055
791.183848	46052.762257	33.075072
792.194953	46110.775035	33.080090
792.647814	46192.848057	33.085108
793.797511	46258.512074	33.090125
794.317036	46343.774311	33.095143
794.886255	46413.547574	33.100160
796.038151	46477.760775	33.105178
796.668056	46555.472362	33.110196
797.526980	46630.201054	33.115213
798.336882	46714.481833	33.120231
798.844082	46785.774554	33.125248
799.928330	46852.047518	33.130266
800.461159	46951.104493	33.135284
801.522801	47026.373675	33.140301
802.409367	47103.046669	33.145319
803.047093	47176.973640	33.150336
803.894036	47250.810828	33.155354
804.783208	47326.645120	33.160372
805.414932	47407.218740	33.165389
806.413828	47480.824468	33.170407
807.167855	47575.867929	33.175424
808.370319	47649.337840	33.180442
808.928098	47725.447460	33.185460
809.790720	47800.871531	33.190477
810.476528	47879.078592	33.195495
811.173511	47964.405627	33.200512
812.096131	48044.516210	33.205530
813.056755	48137.346368	33.210548
813.818100	48203.486502	33.215565
814.697232	48290.325905	33.220583
815.520625	48386.403943	33.225600
816.488274	48457.532322	33.230618
817.118280	48529.705510	33.235636
818.122591	48608.199571	33.240653
819.275873	48681.738407	33.245671
819.934634	48770.177155	33.250688
820.662934	48831.569715	33.255706
821.544393	48923.593037	33.260724
822.369653	48988.548961	33.265741
823.483190	49068.103681	33.270759
823.753337	49136.767801	33.275776
824.932091	49227.290714	33.280794
825.135002	49305.953282	33.285812
826.312896	49384.233825	33.290829
827.106587	49459.455053	33.295847
828.035424	49553.761854	33.300864
828.526953	49629.877578	33.305882
829.601222	49710.432270	33.310900
830.452064	49805.159885	33.315917
831.145291	49883.406164	33.320935
831.672965	49951.025804	33.325952
832.942299	50028.991696	33.330970
833.583730	50101.870002	33.335988
834.367751	50181.330681	33.341005
835.322850	50256.283447	33.346023
836.115171	50319.485464	33.351040
836.734927	50411.662274	33.356058
837.499898	50479.315575	33.361076
838.278998	50552.703970	33.366093
838.953472	50631.679175	33.371111
839.879389	50718.832262	33.376128
840.642850	50793.120364	33.381146
841.300930	50891.406248	33.386164
842.152553	50980.144008	33.391181
843.181811	51063.088284	33.396199
843.790529	51143.676206	33.401216
844.466702	51237.394641	33.406234
845.689916	51324.998832	33.411252
846.410787	51417.000623	33.416269
847.256279	51519.400619	33.421287
847.584390	51608.259520	33.426304
849.271494	51675.180433	33.431322
849.677950	51784.115116	33.436340
850.555661	51882.756500	33.441357
851.876030	51955.237641	33.446375
852.566765	52057.801041	33.451392
853.687018	52139.934198	33.456410
854.517880	52239.288780	33.461428
855.379342	52316.344882	33.466445
856.572371	52404.823898	33.471463
856.972168	52503.535275	33.476480
858.207486	52571.755985	33.481498
858.984760	52654.280616	33.486516
859.925195	52751.127278	33.491533
861.012293	52824.381262	33.496551
861.497715	52922.914031	33.501568
862.456565	53012.244423	33.506586
863.150874	53106.402094	33.511604
864.190732	53180.959071	33.516621
865.423745	53264.499688	33.521639
865.915289	53352.552124	33.526656
867.196056	53424.215403	33.531674
867.853550	53524.232733	33.536692
868.886196	53604.839950	33.541709
869.784016	53682.480004	33.546727
870.589121	53789.570584	33.551744
871.317340	53862.033692	33.556762
872.035435	53945.523677	33.561780
872.764193	54018.416582	33.566797
873.863499	54117.760862	33.571815
874.271254	54222.398472	33.576832
875.470264	54305.179151	33.581850
876.442544	54388.517092	33.586868
877.169159	54487.521843	33.591885
878.015193	54567.222426	33.596903
879.031201	54660.831945	33.601920
879.967116	54729.600846	33.606938
881.009069	54814.769860	33.611956
881.894902	54898.985610	33.616973
882.695082	54965.545378	33.621991
883.474435	55047.010521	33.627008
884.414963	55121.796455	33.632026
885.040184	55204.230625	33.637044
885.798121	55276.833527	33.642061
886.753700	55364.007471	33.647079
887.392361	55452.008779	33.652096
888.487945	55535.600655	33.657114
889.265257	55624.534017	33.662132
890.106994	55709.022520	33.667149
891.256033	55794.949283	33.672167
891.626475	55895.138948	33.677184
892.817492	55971.160627	33.682202
893.832514	56064.600730	33.687220
894.164710	56159.204301	33.692237
895.318850	56255.969332	33.697255
895.955026	56344.720307	33.702272
897.103702	56438.684004	33.707290
898.034723	56542.841251	33.712308
899.038628	56635.916693	33.717325
899.907680	56722.312209	33.722343
900.603955	56822.464554	33.727360
901.522852	56914.800459	33.732378
902.759965	57014.293246	33.737396
903.270782	57120.894572	33.742413
904.523119	57211.540501	33.747431
905.645330	57306.851360	33.752448
907.065476	57407.983986	33.757466
907.681924	57488.466218	33.762484
908.426256	57585.600208	33.767501
909.814472	57663.583228	33.772519
910.359431	57762.931326	33.777536
911.490801	57856.788211	33.782554
912.061044	57957.329825	33.787572
912.921384	58034.236633	33.792589
913.728223	58126.804799	33.797607
914.796254	58231.521208	33.802624
915.767146	58330.397318	33.807642
916.655029	58431.639187	33.812660
917.254176	58530.389249	33.817677
918.656958	58613.605268	33.822695
918.986629	58718.937583	33.827712
920.331634	58814.438607	33.832730
921.466682	58909.651502	33.837748
922.088039	59002.556641	33.842765
923.115915	59104.663915	33.847783
924.100710	59195.535787	33.852800
925.063077	59294.481535	33.857818
926.038819	59391.689198	33.862836
926.519853	59491.119862	33.867853
927.692806	59582.061558	33.872871
928.830991	59681.265540	33.877888
929.737746	59765.787520	33.882906
930.859831	59860.407457	33.887924
931.380820	59941.916387	33.892941
932.710259	60036.520011	33.897959
933.434168	60130.276411	33.902976
934.432399	60217.580151	33.907994
935.075638	60299.036456	33.913012
935.649181	60395.372441	33.918029
937.071502	60476.456123	33.923047
937.805598	60565.309605	33.928064
938.655694	60659.247497	33.933082
939.751749	60750.229223	33.938100
940.354064	60839.420720	33.943117
941.343588	60921.487707	33.948135
941.868455	61007.683231	33.953152
942.961567	61105.635782	33.958170
943.899604	61215.135406	33.963188
944.623854	61324.524434	33.968205
945.776189	61427.218220	33.973223
946.406653	61534.296252	33.978240
947.339035	61638.826022	33.983258
948.578945	61744.043171	33.988276
949.308664	61857.536197	33.993293
950.424538	61966.162487	33.998311
951.560689	62076.178719	34.003328
952.735516	62176.991033	34.008346
953.385570	62280.985108	34.013364
954.143023	62395.711628	34.018381
955.799490	62495.182756	34.023399
956.530191	62602.317214	34.028416
957.327999	62707.164831	34.033434
958.664205	62810.462142	34.038452
959.436228	62925.385341	34.043469
960.942964	63017.256876	34.048487
961.750770	63126.753579	34.053504
962.760722	63221.960908	34.058522
963.617239	63331.132094	34.063540
964.775559	63434.290584	34.068557
965.772937	63520.191872	34.073575
966.640244	63631.567306	34.078592
967.273141	63727.105584	34.083610
968.683667	63827.229174	34.088628
969.488581	63936.866800	34.093645
970.636708	64035.798457	34.098663
971.507819	64134.673645	34.103680
972.218197	64233.240164	34.108698
973.750248	64348.107894	34.113716
974.354386	64452.089587	34.118733
975.566171	64532.428369	34.123751
976.497693	64641.074050	34.128768
977.127054	64750.693754	34.133786
978.634352	64846.979652	34.138804
979.268356	64951.433033	34.143821
980.579229	65057.667895	34.148839
981.798690	65153.634783	34.153856
982.691153	65231.393368	34.158874
983.333915	65321.376441	34.163892
984.271038	65422.862809	34.168909
985.708828	65518.398852	34.173927
986.247397	65609.451554	34.178944
986.887651	65703.264649	34.183962
987.979310	65796.624233	34.188980
988.701670	65896.943960	34.193997
989.689195	65968.433773	34.199015
990.573694	66079.956548	34.204032
991.320940	66174.083388	34.209050
992.452083	66261.396990	34.214068
993.422500	66387.256420	34.219085
994.578100	66496.202279	34.224103
995.461511	66593.992230	34.229120
996.084419	66694.404578	34.234138
997.368557	66806.224885	34.239156
998.513972	66917.692049	34.244173
999.110294	67031.859297	34.249191
1000.189271	67142.747688	34.254208
1001.001520	67252.712632	34.259226
1002.489846	67362.747528	34.264244
1003.207342	67484.156547	34.269261
1004.496424	67597.244079	34.274279
1005.838179	67707.733824	34.279296
1006.601653	67821.879138	34.284314
1007.797012	67917.705707	34.289332
1008.540295	68037.762185	34.294349
1009.657246	68140.027068	34.299367
1010.588331	68257.149032	34.304384
1011.665109	68383.876329	34.309402
1012.661474	68485.479927	34.314420
1013.818105	68600.552799	34.319437
1014.944229	68722.340460	34.324455
1016.009228	68828.685744	34.329472
1016.754703	68935.619436	34.334490
1018.001665	69047.281688	34.339508
1019.110982	69163.098258	34.344525
1020.025448	69285.131588	34.349543
1020.885981	69393.167725	34.354560
1021.842445	69509.642442	34.359578
1022.993487	69619.111984	34.364596
1023.888163	69737.208940	34.369613
1024.937411	69862.598187	34.374631
1026.154206	69970.069083	34.379648
1027.261932	70092.733773	34.384666
1028.334455	70192.167056	34.389684
1029.264410	70318.633309	34.394701
1030.771034	70424.935975	34.399719
1031.555319	70543.617656	34.404736
1032.566028	70655.238206	34.409754
1033.969889	70764.743427	34.414772
1034.659164	70874.236562	34.419789
1035.631044	70971.844867	34.424807
1036.654794	71091.553233	34.429824
1037.516069	71196.793836	34.434842
1038.681081	71301.999322	34.439860
1039.450252	71393.013959	34.444877
1040.586908	71506.622239	34.449895
1041.584705	71610.124707	34.454912
1042.478118	71716.759357	34.459930
1043.410795	71820.121639	34.464948
1044.377508	71930.606425	34.469965
1045.098262	72031.412894	34.474983
1046.554092	72147.021319	34.480000
1047.388537	72257.813309	34.485018
1048.536705	72376.947301	34.490036
1049.884616	72486.256132	34.495053
1050.951556	72591.364018	34.500071
1051.808839	72707.134105	34.505088
1052.727920	72824.411567	34.510106
1054.413076	72938.629570	34.515124
1055.133496	73052.388744	34.520141
1056.010214	73175.823359	34.525159
1057.253700	73272.976431	34.530176
1057.926554	73411.882317	34.535194
1059.191127	73521.595559	34.540212
1060.107036	73645.001567	34.545229
1061.082861	73770.920160	34.550247
1062.071069	73881.178551	34.555264
1063.173231	73999.185787	34.560282
1064.621929	74122.219310	34.565300
1065.732334	74259.279445	34.570317
1066.799231	74375.784189	34.575335
1068.281460	74496.267971	34.580352
1068.906737	74606.038291	34.585370
1070.085874	74727.367920	34.590388
1071.111548	74849.550549	34.595405
1072.553335	74966.517296	34.600423
1073.859020	75085.218982	34.605440
1074.628524	75206.964238	34.610458
1075.835543	75312.083109	34.615476
1077.106698	75433.111657	34.620493
1077.888740	75546.394888	34.625511
1079.140928	75669.007804	34.630528
1080.054650	75785.456601	34.635546
1081.168314	75898.025479	34.640564
1082.282577	76030.091744	34.645581
1083.499193	76139.321330	34.650599
1084.852897	76260.828347	34.655616
1085.676321	76369.571877	34.660634
1087.125544	76484.182568	34.665652
1087.719334	76599.795812	34.670669
1089.091813	76720.733797	34.675687
1090.319490	76818.867188	34.680704
1091.495560	76942.688117	34.685722
1092.395242	77046.569254	34.690740
1093.163431	77166.164996	34.695757
1094.100220	77294.791591	34.700775
1095.724787	77409.594512	34.705792
1096.170050	77529.711453	34.710810
1097.624754	77627.553507	34.715828
1098.440099	77742.493329	34.720845
1099.310968	77844.379545	34.725863
1100.494379	77961.537425	34.730880
1101.304897	78077.023460	34.735898
1102.523052	78191.623642	34.740916
1103.466130	78303.417627	34.745933
1104.597129	78423.418119	34.750951
1105.883054	78544.772581	34.755968
1106.810333	78660.767956	34.760986
1107.859100	78769.450531	34.766004
1108.952831	78897.158387	34.771021
1109.601950	79029.849025	34.776039
1111.437798	79149.299211	34.781056
1112.330860	79278.887046	34.786074
1113.596659	79388.214717	34.791092
1114.667802	79519.324372	34.796109
1115.657165	79658.165823	34.801127
1116.925677	79768.380024	34.806144
1118.065552	79907.262427	34.811162
1118.931919	80031.638023	34.816180
1119.965502	80150.507326	34.821197
1121.157823	80295.262680	34.826215
1123.045114	80416.760115	34.831232
1124.291635	80547.431210	34.836250
1125.339428	80660.909134	34.841268
1126.499781	80786.810206	34.846285
1127.417302	80909.798570	34.851303
1128.604043	81030.981169	34.856320
1129.394717	81168.789715	34.861338
1130.892118	81285.360292	34.866356
1132.139703	81399.088629	34.871373
1132.742365	81547.973326	34.876391
1134.290661	81678.357011	34.881408
1135.382897	81798.187320	34.886426
1136.666355	81920.680953	34.891444
1137.985269	82046.962711	34.896461
1139.001116	82181.208297	34.901479
1139.772474	82300.175861	34.906496
1141.010142	82433.395266	34.911514
1142.290677	82549.899939	34.916532
1143.567896	82690.612459	34.921549
1144.531198	82809.963324	34.926567
1145.869832	82942.967615	34.931584
1146.691474	83083.489697	34.936602
1147.973469	83206.528472	34.941620
1149.369680	83333.336760	34.946637
1150.165531	83464.135739	34.951655
1151.499097	83593.168316	34.956672
1152.434279	83715.038713	34.961690
1153.558301	83861.144703	34.966708
1155.038402	83977.789950	34.971725
1155.751423	84127.193847	34.976743
1157.053765	84246.132254	34.981760
1158.224285	84373.785645	34.986778
1159.351816	84490.546697	34.991796
1160.497233	84619.172901	34.996813
1161.182151	84734.545183	35.001831
1162.510951	84856.144610	35.006848
1163.682884	84980.501051	35.011866
1165.046115	85111.182074	35.016884
1166.440963	85231.698303	35.021901
1167.260185	85362.505316	35.026919
1168.650306	85479.090963	35.031936
1169.786394	85612.093709	35.036954
1170.668435	85734.319297	35.041972
1172.181853	85862.009324	35.046989
1173.093297	85986.084285	35.052007
1174.496799	86118.358476	35.057024
1175.301473	86245.942200	35.062042
1176.684055	86387.693236	35.067060
1177.543635	86511.874348	35.072077
1178.678931	86651.769536	35.077095
1179.813756	86793.632216	35.082112
1181.011469	86925.558416	35.087130
1182.050769	87064.402945	35.092148
1183.200603	87220.057045	35.097165
1184.432693	87357.456401	35.102183
1185.862260	87490.632847	35.107200
1186.983245	87642.437346	35.112218
1188.148856	87794.665816	35.117236
1189.341940	87928.167130	35.122253
1190.674354	88071.967121	35.127271
1192.030366	88226.413222	35.132288
1193.360485	88366.313895	35.137306
1194.499697	88510.400474	35.142324
1195.748446	88650.562550	35.147341
1197.148825	88783.637805	35.152359
1198.602756	88920.942298	35.157376
1199.548525	89062.584393	35.162394
1200.783701	89183.192505	35.167412
1202.255235	89336.565761	35.172429
1203.357020	89471.311638	35.177447
1204.394445	89592.883090	35.182464
1205.701482	89745.697261	35.187482
1206.926003	89882.544720	35.192500
1208.137120	90024.258404	35.197517
1209.313677	90166.402223	35.202535
1210.940739	90298.900528	35.207552
1212.187337	90435.159800	35.212570
1212.991651	90574.197027	35.217588
1214.244002	90709.192242	35.222605
1215.463256	90856.627205	35.227623
1216.947862	90982.423211	35.232640
1218.236318	91127.104214	35.237658
1219.689672	91250.199876	35.242676
1220.625558	91390.372417	35.247693
1221.969352	91529.823247	35.252711
1223.234389	91644.501486	35.257728
1224.681281	91779.333223	35.262746
1225.677313	91902.663371	35.267764
1227.127044	92007.257960	35.272781
1228.097686	92119.601082	35.277799
1229.456768	92236.013073	35.282816
1230.601035	92367.392624	35.287834
1231.745461	92470.709752	35.292852
1233.063788	92590.166000	35.297869
1233.870778	92732.789992	35.302887
1235.075175	92835.605952	35.307904
1236.656205	92961.037430	35.312922
1237.225169	93103.689004	35.317940
1238.651071	93221.702115	35.322957
1239.780721	93366.081517	35.327975
1241.003944	93502.325552	35.332992
1242.039282	93628.170143	35.338010
1242.571208	93769.446676	35.343028
1244.241344	93920.865903	35.348045
1245.628124	94073.533010	35.353063
1246.893020	94222.203972	35.358080
1248.086171	94369.476780	35.363098
1249.234862	94516.694373	35.368116
1250.703196	94657.245723	35.373133
1251.901581	94809.017975	35.378151
1253.096726	94949.013671	35.383168
1254.373183	95106.272396	35.388186
1255.753271	95245.127243	35.393204
1257.266630	95388.111379	35.398221
1258.402594	95535.565418	35.403239
1259.978110	95689.605201	35.408256
1261.265932	95822.949615	35.413274
1262.503700	95985.129433	35.418292
1263.821034	96127.630722	35.423309
1265.055093	96273.195226	35.428327
1266.337269	96416.412429	35.433344
1267.588730	96570.300996	35.438362
1268.560414	96711.260452	35.443380
1270.041869	96853.322716	35.448397
1271.033618	97008.463826	35.453415
1272.879551	97161.433193	35.458432
1274.179832	97311.377861	35.463450
1274.978185	97461.953691	35.468468
1276.622235	97600.350893	35.473485
1278.056851	97754.123490	35.478503
1279.059311	97901.183994	35.483520
1280.370000	98055.263011	35.488538
1281.660063	98196.060871	35.493556
1283.216111	98327.454165	35.498573
1284.390755	98496.507203	35.503591
1285.691423	98628.727315	35.508608
1287.052292	98779.912021	35.513626
1288.072530	98923.667485	35.518644
1289.712705	99070.058419	35.523661
1291.000124	99221.820792	35.528679
1292.155324	99374.655425	35.533696
1293.624366	99516.774232	35.538714
1294.714259	99646.673834	35.543732
1296.081573	99770.298123	35.548749
1297.459775	99904.063343	35.553767
1298.676342	100035.805112	35.558784
1299.564926	100166.897477	35.563802
1300.751704	100301.720402	35.568820
1301.987203	100451.866775	35.573837
1303.097336	100592.682633	35.578855
1304.108761	100734.527376	35.583872
1305.522711	100881.731375	35.588890
1306.565777	101046.844285	35.593908
1308.289757	101186.712008	35.598925
1309.398651	101340.636321	35.603943
1310.814120	101497.391852	35.608960
1312.218921	101646.196641	35.613978
1313.251150	101804.299614	35.618996
1314.631351	101963.803660	35.624013
1315.882063	102116.495691	35.629031
1317.474131	102276.297228	35.634048
1318.666854	102445.091547	35.639066
1319.689270	102607.624497	35.644084
1321.503080	102752.802554	35.649101
1322.627005	102921.282204	35.654119
1323.895128	103085.481566	35.659136
1325.440224	103244.183494	35.664154
1326.701523	103417.529927	35.669172
1328.145014	103574.851786	35.674189
1329.626782	103742.299623	35.679207
1330.831349	103897.668318	35.684224
1332.116967	104065.206578	35.689242
1333.498241	104240.128325	35.694260
1334.979582	104384.799782	35.699277
1336.292974	104551.185359	35.704295
1337.766079	104724.482416	35.709312
1339.088625	104878.902236	35.714330
1340.680145	105044.329476	35.719348
1342.095133	105202.989314	35.724365
1343.474996	105357.314540	35.729383
1344.587992	105514.809413	35.734400
1346.183331	105671.462922	35.739418
1347.317410	105844.727107	35.744436
1349.001680	106006.001134	35.749453
1350.455965	106162.230961	35.754471
1351.482203	106316.916046	35.759488
1353.175916	106478.210746	35.764506
1354.453555	106643.344568	35.769524
1355.894772	106801.517228	35.774541
1357.523034	106950.617375	35.779559
1358.716593	107102.654493	35.784576
1360.126166	107264.265452	35.789594
1361.538838	107417.491207	35.794612
1362.932882	107567.385545	35.799629
1364.533449	107715.861947	35.804647
1365.431213	107879.001380	35.809664
1366.897083	108029.121346	35.814682
1367.949813	108167.415528	35.819700
1369.531878	108305.012446	35.824717
1370.653649	108456.392288	35.829735
1371.898883	108595.974791	35.834752
1373.343575	108731.855434	35.839770
1374.084525	108890.558154	35.844788
1375.657419	109039.692664	35.849805
1377.188667	109201.176971	35.854823
1378.231877	109354.030646	35.859840
1380.034224	109492.491735	35.864858
1380.597737	109672.380754	35.869876
1381.772313	109834.331027	35.874893
1383.675279	109994.444969	35.879911
1384.747702	110147.716720	35.884928
1386.448908	110318.175787	35.889946
1387.729480	110502.318078	35.894964
1389.348309	110660.158529	35.899981
1390.832409	110824.591724	35.904999
1391.641682	111003.818471	35.910016
1393.400629	111174.267974	35.915034
1394.448266	111340.451395	35.920052
1396.094663	111508.066300	35.925069
1397.436952	111699.816352	35.930087
1398.791917	111871.145111	35.935104
1400.406642	112052.150479	35.940122
1401.695643	112226.847135	35.945140
1403.519688	112405.422693	35.950157
1405.132312	112577.937118	35.955175
1406.463223	112754.871731	35.960192
1408.223226	112917.230314	35.965210
1409.615114	113084.833023	35.970228
1410.789314	113255.218847	35.975245
1412.478891	113426.505153	35.980263
1413.804958	113592.317550	35.985280
1415.453295	113753.053390	35.990298
1416.902171	113932.313569	35.995316
1418.276402	114093.367366	36.000333
1419.981471	114263.637710	36.005351
1421.191624	114433.601682	36.010368
1422.503250	114599.758561	36.015386
1423.853833	114770.101326	36.020404
1425.489553	114947.059967	36.025421
1426.692540	115118.055290	36.030439
1427.938349	115277.465718	36.035456
1429.981959	115443.024353	36.040474
1431.433345	115629.279255	36.045492
1432.649789	115789.267364	36.050509
1434.316759	115951.894594	36.055527
1435.569947	116128.745014	36.060544
1437.093211	116288.598878	36.065562
1438.570550	116459.825562	36.070580
1440.326400	116621.119728	36.075597
1441.654406	116780.741796	36.080615
1442.841566	116953.657710	36.085632
1444.455926	117104.505395	36.090650
1445.598578	117263.729399	36.095668
1447.149225	117422.560328	36.100685
1448.586860	117559.325984	36.105703
1450.141252	117715.017717	36.110720
1451.356925	117861.589789	36.115738
1452.755466	118028.540368	36.120756
1453.909110	118171.850630	36.125773
1455.398988	118331.823869	36.130791
1456.826391	118496.632792	36.135808
1458.412751	118651.761590	36.140826
1459.420509	118823.471235	36.145844
1460.875453	118993.717961	36.150861
1462.476175	119150.715362	36.155879
1464.212591	119320.900520	36.160896
1465.601865	119488.482532	36.165914
1466.864324	119654.262161	36.170932
1468.185210	119831.310918	36.175949
1469.744131	119998.489339	36.180967
1471.120439	120194.490003	36.185984
1473.036379	120355.009579	36.191002
1474.633907	120533.817484	36.196020
1476.142793	120703.180317	36.201037
1477.675180	120874.769476	36.206055
1479.330668	121042.084875	36.211072
1480.520314	121209.323379	36.216090
1482.142551	121386.790716	36.221108
1483.857646	121551.275633	36.226125
1485.364010	121723.393733	36.231143
1486.667317	121896.393778	36.236160
1488.235628	122064.578091	36.241178
1490.234512	122243.004565	36.246196
1491.140740	122410.283051	36.251213
1493.045592	122580.013004	36.256231
1494.393231	122755.392718	36.261248
1495.755340	122929.327418	36.266266
1497.144687	123099.205923	36.271284
1498.625610	123277.886308	36.276301
1500.250131	123447.919661	36.281319
1501.986483	123628.930325	36.286336
1503.447759	123793.456821	36.291354
1504.966734	123972.249806	36.296372
1506.018355	124147.533718	36.301389
1508.030898	124323.058764	36.306407
1509.348998	124503.153827	36.311424
1510.915066	124685.097996	36.316442
1512.328356	124864.217710	36.321460
1513.964825	125048.040453	36.326477
1515.395185	125219.331882	36.331495
1517.226567	125396.172048	36.336512
1518.752515	125573.961239	36.341530
1520.342211	125740.746612	36.346548
1521.608137	125929.422306	36.351565
1523.303929	126092.367562	36.356583
1524.323689	126273.395855	36.361600
1526.008458	126450.620878	36.366618
1527.718357	126603.445855	36.371636
1529.119283	126770.596894	36.376653
1530.949566	126916.551460	36.381671
1532.259790	127082.300066	36.386688
1533.605949	127238.885304	36.391706
1535.334281	127394.942023	36.396724
1536.486026	127574.564537	36.401741
1538.118105	127722.125694	36.406759
1539.365321	127904.091410	36.411776
1540.360007	128068.755998	36.416794
1541.933067	128246.909833	36.421812
1543.457449	128426.301363	36.426829
1545.240355	128612.734521	36.431847
1546.503452	128798.035358	36.436864
1548.161074	128975.306350	36.441882
1549.764923	129165.255485	36.446900
1551.307316	129346.030983	36.451917
1553.308986	129534.804621	36.456935
1554.700693	129720.711956	36.461952
1556.241194	129910.650915	36.466970
1557.715331	130091.404095	36.471988
1559.342724	130283.080094	36.477005
1560.799056	130472.263438	36.482023
1562.393921	130669.255589	36.487040
1564.268562	130858.514455	36.492058
1565.693653	131052.330950	36.497076
1567.413875	131243.682043	36.502093
1569.015616	131426.045251	36.507111
1570.463770	131619.114487	36.512128
1572.316661	131816.086358	36.517146
1573.830920	132000.228259	36.522164
1575.329101	132193.255464	36.527181
1577.597951	132371.654515	36.532199
1578.795440	132573.765725	36.537216
1580.136833	132753.860242	36.542234
1582.021437	132942.079880	36.547252
1583.581477	133137.675725	36.552269
1585.318602	133331.711672	36.557287
1586.935388	133521.409427	36.562304
1588.563741	133715.325884	36.567322
1590.118010	133899.942535	36.572340
1591.280084	134098.218306	36.577357
1593.154308	134273.270862	36.582375
1594.657139	134478.223302	36.587392
1596.371834	134662.439248	36.592410
1598.065480	134856.251670	36.597428
1599.511901	135054.957692	36.602445
1601.335690	135240.237043	36.607463
1603.506291	135433.597447	36.612480
1605.033619	135615.276963	36.617498
1606.952074	135796.211237	36.622516
1608.314862	135987.790259	36.627533
1610.279975	136153.323472	36.632551
1611.680191	136342.846090	36.637568
1613.212623	136510.122713	36.642586
1614.961427	136674.071259	36.647604
1616.224742	136840.923664	36.652621
1617.649960	137003.835672	36.657639
1619.027062	137167.085701	36.662656
1620.710372	137326.156905	36.667674
1622.563342	137508.645515	36.672692
1623.930145	137681.999757	36.677709
1625.362577	137848.387497	36.682727
1626.501653	138028.052736	36.687744
1628.103675	138204.958977	36.692762
1630.012392	138393.742427	36.697780
1631.221407	138584.158924	36.702797
1632.895624	138761.601949	36.707815
1634.708748	138948.896066	36.712832
1636.137589	139153.804310	36.717850
1637.780345	139341.165973	36.722868
1639.451771	139539.106238	36.727885
1641.268907	139729.775653	36.732903
1642.678935	139926.074472	36.737920
1644.064524	140130.882228	36.742938
1646.074414	140318.787353	36.747956
1647.491229	140542.742408	36.752973
1649.185694	140731.422595	36.757991
1650.985421	140943.723540	36.763008
1652.903697	141144.626163	36.768026
1654.359608	141346.085155	36.773044
1655.934129	141555.283062	36.778061
1657.700072	141758.723380	36.783079
1659.745578	141958.787391	36.788096
1661.379383	142168.879967	36.793114
1662.964676	142358.791672	36.798132
1664.463436	142576.196172	36.803149
1666.418262	142774.797049	36.808167
1668.059279	142979.684887	36.813184
1669.654893	143182.021046	36.818202
1671.468750	143391.992035	36.823220
1673.058159	143600.694605	36.828237
1674.890862	143805.772982	36.833255
1676.804714	144013.945184	36.838272
1678.251518	144219.708664	36.843290
1680.256107	144417.729197	36.848308
1682.153169	144614.842788	36.853325
1683.632756	144816.346176	36.858343
1685.497982	145020.806353	36.863360
1687.265447	145229.415573	36.868378
1689.059507	145425.701409	36.873396
1690.237914	145628.639502	36.878413
1692.528036	145822.047758	36.883431
1694.161722	146030.506110	36.888448
1695.532844	146234.545662	36.893466
1697.730678	146424.524475	36.898484
1699.190002	146621.631506	36.903501
1700.693913	146834.400265	36.908519
1702.669403	147021.806724	36.913536
1704.259199	147223.713717	36.918554
1705.865162	147404.881058	36.923572
1707.289415	147593.189712	36.928589
1709.323517	147757.761144	36.933607
1711.148008	147948.784484	36.938624
1712.401367	148131.000720	36.943642
1714.157182	148301.348954	36.948660
1715.870604	148485.053382	36.953677
1717.213027	148673.964542	36.958695
1718.765313	148861.588485	36.963712
1720.291498	149068.917600	36.968730
1721.995032	149256.557865	36.973748
1723.497184	149465.592069	36.978765
1725.256532	149663.735142	36.983783
1727.222173	149877.211485	36.988800
1728.862675	150083.502114	36.993818
1730.795602	150281.431250	36.998836
1732.460507	150494.287510	37.003853
1734.284303	150707.373484	37.008871
1736.034387	150917.924351	37.013888
1737.367804	151122.685626	37.018906
1739.296040	151327.303027	37.023924
1741.041256	151546.581046	37.028941
1742.859312	151757.380081	37.033959
1744.976545	151979.454468	37.038976
1746.473847	152206.205593	37.043994
1748.026127	152414.895755	37.049012
1749.958974	152631.412715	37.054029
1751.509849	152847.890313	37.059047
1753.496132	153072.338343	37.064064
1755.211358	153292.025755	37.069082
1757.163523	153514.846657	37.074100
1759.202799	153733.674100	37.079117
1761.031783	153945.093907	37.084135
1762.990463	154165.635936	37.089152
1764.973832	154384.222936	37.094170
1766.865721	154586.178293	37.099188
1768.184896	154809.311177	37.104205
1770.360922	155016.878899	37.109223
1772.041161	155219.746524	37.114240
1774.247853	155427.540132	37.119258
1775.964230	155648.409287	37.124276
1777.613363	155860.630440	37.129293
1779.320206	156068.063547	37.134311
1781.186418	156270.121794	37.139328
1782.791668	156496.136684	37.144346
1784.673621	156704.864558	37.149364
1786.721464	156915.748314	37.154381
1788.267410	157124.253131	37.159399
1790.187807	157329.529748	37.164416
1791.526334	157547.960515	37.169434
1793.685785	157770.079085	37.174452
1795.333291	157983.264661	37.179469
1797.316863	158179.964424	37.184487
1799.235169	158402.290183	37.189504
1800.629885	158610.916743	37.194522
1802.619349	158797.576090	37.199540
1804.048485	158988.281761	37.204557
1805.471360	159191.606805	37.209575
1807.566861	159381.752330	37.214592
1809.322770	159582.579380	37.219610
1810.888153	159780.090053	37.224628
1812.610477	159992.109382	37.229645
1814.294557	160200.598030	37.234663
1816.235986	160406.929299	37.239680
1817.822498	160625.999374	37.244698
1819.679230	160824.661682	37.249716
1821.563595	161038.665218	37.254733
1823.128795	161262.789807	37.259751
1825.288069	161478.553121	37.264768
1826.754078	161702.036776	37.269786
1828.611644	161930.709904	37.274804
1830.695259	162141.936495	37.279821
1832.195000	162366.611029	37.284839
1834.375005	162584.140496	37.289856
1835.986032	162832.921359	37.294874
1838.030338	163052.935511	37.299892
1839.945098	163277.245465	37.304909
1841.986161	163507.865214	37.309927
1844.029567	163730.635678	37.314944
1845.610561	163966.074563	37.319962
1847.836616	164175.717802	37.324980
1849.649782	164402.536590	37.329997
1851.407968	164641.223804	37.335015
1853.433423	164860.972850	37.340032
1855.359628	165093.168131	37.345050
1857.333502	165317.202201	37.350068
1859.458381	165536.254617	37.355085
1861.383955	165761.465880	37.360103
1863.287268	165978.805822	37.365120
1865.141568	166203.320825	37.370138
1867.068491	166414.191130	37.375156
1868.971471	166637.140978	37.380173
1870.620464	166874.477428	37.385191
1872.711029	167083.702057	37.390208
1874.363436	167310.970027	37.395226
1876.353750	167537.285197	37.400244
1878.226689	167759.345938	37.405261
1880.035888	167999.073961	37.410279
1881.846383	168224.445135	37.415296
1883.885596	168446.483516	37.420314
1885.862275	168671.310924	37.425332
1887.797696	168894.662165	37.430349
1889.321329	169129.597311	37.435367
1891.420442	169347.483703	37.440384
1893.383589	169585.535635	37.445402
1895.444789	169813.096154	37.450420
1897.060802	170041.261424	37.455437
1899.057041	170261.642798	37.460455
1901.121229	170484.196400	37.465472
1902.777786	170710.735550	37.470490
1904.825129	170921.599039	37.475508
1906.898366	171113.800164	37.480525
1908.231099	171327.443082	37.485543
1910.061942	171526.344285	37.490560
1912.017698	171736.249970	37.495578
1913.687277	171950.743465	37.500596
1916.019096	172158.676274	37.505613
1917.590110	172376.460507	37.510631
1919.869524	172576.843437	37.515648
1921.271400	172803.473155	37.520666
1923.440338	173012.146690	37.525684
1925.653750	173235.580204	37.530701
1927.132003	173446.712456	37.535719
1929.152991	173672.614591	37.540736
1931.107963	173897.221850	37.545754
1932.562842	174117.127188	37.550772
1934.468274	174355.305991	37.555789
1936.453187	174584.428512	37.560807
1938.805090	174814.813439	37.565824
1940.353935	175059.167647	37.570842
1942.322160	175291.328796	37.575860
1944.527384	175528.299805	37.580877
1946.418813	175772.426325	37.585895
1948.550558	176005.149165	37.590912
1951.003484	176247.020043	37.595930
1952.634422	176482.920567	37.600948
1954.745097	176716.627650	37.605965
1956.879745	176948.898660	37.610983
1959.209117	177167.971235	37.616000
1961.318542	177398.142772	37.621018
1963.332803	177634.458453	37.626036
1965.400609	177851.279817	37.631053
1967.196760	178074.780727	37.636071
1969.319411	178299.423608	37.641088
1971.582318	178534.943705	37.646106
1973.223013	178760.211080	37.651124
1975.426872	178972.703004	37.656141
1977.512747	179203.509889	37.661159
1979.638535	179426.775369	37.666176
1981.375266	179649.164886	37.671194
1983.141752	179878.770066	37.676212
1985.480579	180105.405574	37.681229
1987.566747	180326.690108	37.686247
1989.210833	180550.875305	37.691264
1991.563029	180776.712920	37.696282
1993.340323	181000.118055	37.701300
1995.485781	181214.520920	37.706317
1997.373915	181446.779660	37.711335
1999.544586	181675.353334	37.716352
2001.375927	181910.376884	37.721370
2003.398872	182138.253206	37.726388
2005.273966	182345.649908	37.731405
2007.072101	182590.668070	37.736423
2009.169596	182815.249808	37.741440
2011.209347	183030.921852	37.746458
2013.229564	183245.126182	37.751476
2015.021320	183455.180561	37.756493
2016.555891	183656.052086	37.761511
2018.549663	183874.362095	37.766528
2020.616410	184096.036814	37.771546
2022.665481	184312.804857	37.776564
2024.802018	184518.457282	37.781581
2026.528297	184748.931917	37.786599
2028.309249	184959.464591	37.791616
2030.326389	185183.106674	37.796634
2032.184356	185416.444257	37.801652
2034.243955	185640.576746	37.806669
2036.280417	185883.633738	37.811687
2038.407461	186113.353837	37.816704
2040.331418	186351.456950	37.821722
2042.207876	186596.839915	37.826740
2044.600255	186831.762285	37.831757
2046.670519	187070.543847	37.836775
2048.852870	187316.326258	37.841792
2051.133605	187560.000559	37.846810
2053.196093	187797.657725	37.851828
2055.222112	188035.220373	37.856845
2057.499028	188279.254369	37.861863
2059.859192	188508.023042	37.866880
2062.419866	188733.106283	37.871898
2063.706637	188978.519254	37.876916
2066.235053	189205.284971	37.881933
2068.347738	189451.305404	37.886951
2070.112279	189678.270717	37.891968
2072.439477	189924.348404	37.896986
2074.267354	190165.011611	37.902004
2076.836158	190393.781693	37.907021
2078.915339	190631.691612	37.912039
2080.877807	190868.428305	37.917056
2083.444038	191092.582736	37.922074
2085.804317	191333.116574	37.927092
2088.184538	191558.444844	37.932109
2090.014878	191775.802686	37.937127
2091.834966	192009.978610	37.942144
2094.572056	192236.484429	37.947162
2096.565253	192462.525516	37.952180
2098.786640	192684.102248	37.957197
2100.708268	192900.993726	37.962215
2102.994644	193133.184675	37.967232
2105.245183	193354.975548	37.972250
2107.216530	193586.355587	37.977268
2109.713686	193780.835562	37.982285
2111.855475	194006.910902	37.987303
2113.889416	194232.661700	37.992320
2116.110693	194439.917582	37.997338
2118.144604	194660.212940	38.002356
2120.426844	194885.445002	38.007373
2122.483222	195104.190350	38.012391
2124.165718	195307.778511	38.017408
2126.596330	195508.291624	38.022426
2128.023267	195713.026132	38.027444
2130.485309	195901.529297	38.032461
2132.734312	196098.976711	38.037479
2134.778136	196295.937059	38.042496
2136.729208	196480.880796	38.047514
2138.591476	196696.401887	38.052532
2140.614488	196882.681017	38.057549
2142.537960	197102.103274	38.062567
2144.292326	197304.964489	38.067584
2146.770755	197514.578188	38.072602
2148.696350	197734.040845	38.077620
2150.933340	197946.436121	38.082637
2152.876696	198175.835973	38.087655
2155.035577	198390.822004	38.092672
2157.328889	198615.852803	38.097690
2159.026173	198833.249279	38.102708
2161.549691	199061.570924	38.107725
2163.527112	199298.166979	38.112743
2165.568987	199524.993097	38.117760
2168.066435	199756.253879	38.122778
2170.002843	200009.042957	38.127796
2172.270824	200250.433116	38.132813
2174.115251	200486.306599	38.137831
2176.375606	200716.936363	38.142848
2178.718840	200963.483835	38.147866
2180.928881	201215.016579	38.152884
2182.924023	201449.524838	38.157901
2185.558627	201702.160253	38.162919
2187.780770	201930.554465	38.167936
2190.630674	202173.041286	38.172954
2192.588201	202427.386760	38.177972
2195.111992	202646.952198	38.182989
2197.079572	202890.534084	38.188007
2199.560501	203128.437725	38.193024
2202.180193	203356.825495	38.198042
2203.984344	203611.391058	38.203060
2206.429737	203836.038365	38.208077
2208.471884	204070.981741	38.213095
2211.033292	204306.313407	38.218112
2213.310205	204527.803993	38.223130
2215.131095	204775.326954	38.228148
2217.269172	205011.591835	38.233165
2219.558972	205238.655793	38.238183
2221.798835	205473.510066	38.243200
2224.301472	205719.139068	38.248218
2226.549049	205966.739076	38.253236
2229.026949	206192.647130	38.258253
2231.143442	206421.456898	38.263271
2233.167902	206661.364355	38.268288
2235.530754	206893.488202	38.273306
2237.059269	207126.354599	38.278324
2239.759702	207372.568451	38.283341
2242.210784	207612.069331	38.288359
2244.174679	207861.105936	38.293376
2246.462962	208086.213396	38.298394
2248.170514	208313.571890	38.303412
2250.540561	208517.137701	38.308429
2252.789289	208744.995952	38.313447
2254.499983	208966.478674	38.318464
2256.704813	209178.667325	38.323482
2258.694093	209412.028013	38.328500
2260.938784	209641.857953	38.333517
2263.298374	209870.350239	38.338535
2265.332630	210121.758855	38.343552
2267.660570	210355.310597	38.348570
2269.519731	210592.809581	38.353588
2271.813147	210840.130213	38.358605
2273.783539	211096.859479	38.363623
2276.085690	211354.755935	38.368640
2278.716291	211613.248823	38.373658
2280.603294	211876.773810	38.378676
2283.040829	212127.390110	38.383693
2285.790806	212392.913226	38.388711
2288.128918	212665.244113	38.393728
2290.394200	212918.912352	38.398746
2292.506790	213191.979462	38.403764
2294.924693	213453.979365	38.408781
2297.167274	213703.566202	38.413799
2299.584013	213971.205292	38.418816
2302.153027	214245.169281	38.423834
2304.299610	214509.438166	38.428852
2306.693635	214783.013139	38.433869
2309.561187	215040.796402	38.438887
2311.545206	215315.822416	38.443904
2314.020503	215583.090464	38.448922
2316.555540	215839.748741	38.453940
2318.692185	216110.716363	38.458957
2321.383928	216380.187753	38.463975
2323.285005	216646.446404	38.468992
2325.978809	216910.447395	38.474010
2328.333563	217179.899140	38.479028
2330.409846	217434.096768	38.484045
2332.937583	217705.427583	38.489063
2335.067912	217979.526825	38.494080
2337.945205	218240.977096	38.499098
2340.178305	218526.666899	38.504116
2342.370498	218794.550771	38.509133
2345.235668	219051.536666	38.514151
2347.172656	219335.676823	38.519168
2349.653091	219597.461573	38.524186
2351.820476	219863.880485	38.529204
2354.112904	220143.650472	38.534221
2356.445239	220402.947568	38.539239
2358.523190	220694.625369	38.544256
2361.362568	220959.418044	38.549274
2363.744634	221235.279909	38.554292
2366.214152	221507.230874	38.559309
2368.413663	221786.551943	38.564327
2370.585913	222052.330324	38.569344
2373.273576	222317.164504	38.574362
2375.319974	222578.457098	38.579380
2377.537521	222814.468235	38.584397
2379.811823	223070.621992	38.589415
2381.864726	223307.244809	38.594432
2383.672339	223621.044921	38.599450
2385.872239	223889.009189	38.604468
2388.295520	224155.542212	38.609485
2390.908189	224424.115832	38.614503
2392.591757	224703.287871	38.619520
2395.139366	224976.965448	38.624538
2397.323052	225261.063066	38.629556
2399.800431	225558.917709	38.634573
2402.036899	225838.678995	38.639591
2404.450639	226141.980550	38.644608
2406.880355	226436.747620	38.649626
2409.270355	226733.096586	38.654644
2411.448460	227030.394450	38.659661
2414.452575	227331.346478	38.664679
2416.583555	227634.647457	38.669696
2419.346851	227938.027062	38.674714
2421.670203	228240.842556	38.679732
2424.026435	228548.834813	38.684749
2426.432052	228861.340951	38.689767
2429.110893	229168.166799	38.694784
2431.803238	229467.728057	38.699802
2434.439866	229785.000864	38.704820
2436.439338	230083.327969	38.709837
2439.539782	230395.907152	38.714855
2441.897936	230704.617694	38.719872
2444.460704	231006.769732	38.724890
2447.125613	231315.306726	38.729908
2449.708727	231613.012975	38.734925
2452.604659	231911.305536	38.739943
2454.814352	232221.822498	38.744960
2457.611878	232515.180023	38.749978
2459.939646	232824.867515	38.754996
2462.270750	233121.450157	38.760013
2465.227309	233411.356504	38.765031
2467.108046	233724.876631	38.770048
2470.028598	234022.054347	38.775066
2472.652977	234316.638483	38.780084
2474.970083	234628.543030	38.785101
2477.458819	234919.620081	38.790119
2480.130655	235224.333317	38.795136
2482.955553	235516.400145	38.800154
2485.183998	235813.057884	38.805172
2487.525707	236112.390783	38.810189
2490.006991	236407.638627	38.815207
2492.676014	236714.515604	38.820224
2494.993531	237010.121278	38.825242
2497.612048	237299.381132	38.830260
2500.043219	237605.282415	38.835277
2502.525270	237908.484197	38.840295
2504.713775	238218.718110	38.845312
2507.405261	238495.777994	38.850330
2509.731463	238775.512586	38.855348
2511.952623	239055.823311	38.860365
2514.661470	239324.297524	38.865383
2516.733447	239605.293640	38.870400
2518.905895	239896.510540	38.875418
2521.508165	240176.154045	38.880436
2523.757122	240467.131663	38.885453
2526.129201	240759.639878	38.890471
2528.324114	241059.542831	38.895488
2530.765401	241350.390551	38.900506
2533.320209	241661.083722	38.905524
2535.375845	241974.803187	38.910541
2538.228225	242279.557988	38.915559
2540.746367	242610.427020	38.920576
2543.409121	242931.545746	38.925594
2545.956689	243250.473722	38.930612
2548.220978	243571.987415	38.935629
2550.962208	243893.146935	38.940647
2553.483404	244239.767950	38.945664
2556.082741	244561.789815	38.950682
2558.410843	244896.860525	38.955700
2560.859141	245237.323361	38.960717
2563.867688	245576.250441	38.965735
2566.358224	245915.362040	38.970752
2568.754535	246259.848969	38.975770
2571.807101	246594.224818	38.980788
2574.214457	246944.630070	38.985805
2576.989823	247287.408370	38.990823
2579.513848	247631.167141	38.995840
2582.424261	247976.973785	39.000858
2585.078601	248310.299027	39.005876
2587.505244	248663.118421	39.010893
2590.228315	249004.334076	39.015911
2592.662237	249344.402432	39.020928
2595.368819	249701.396457	39.025946
2598.353263	250051.209450	39.030964
2601.004383	250399.297907	39.035981
2603.747561	250731.115522	39.040999
2606.381276	251080.122630	39.046016
2609.037073	251426.383584	39.051034
2612.049064	251763.698210	39.056052
2614.291200	252104.971125	39.061069
2617.378656	252435.645237	39.066087
2620.115972	252776.256755	39.071104
2622.797029	253122.186825	39.076122
2625.593506	253453.975778	39.081140
2628.056691	253791.381158	39.086157
2630.742412	254125.500424	39.091175
2632.976307	254471.021176	39.096192
2636.071123	254806.854951	39.101210
2639.013608	255127.294312	39.106228
2641.478208	255476.082543	39.111245
2644.338901	255800.600274	39.116263
2646.908265	256132.734542	39.121280
2649.185602	256458.514203	39.126298
2652.029116	256760.555065	39.131316
2654.624474	257053.541596	39.136333
2657.478959	257345.395160	39.141351
2659.826462	257643.934050	39.146368
2662.452991	257945.579036	39.151386
2665.019018	258240.807155	39.156404
2666.825275	258554.877676	39.161421
2669.837060	258863.931146	39.166439
2672.242439	259188.932295	39.171456
2674.558821	259517.529734	39.176474
2676.967379	259844.106177	39.181492
2679.228149	260175.177312	39.186509
2681.860619	260521.584041	39.191527
2684.541879	260865.443198	39.196544
2686.872088	261224.092011	39.201562
2689.659974	261581.042989	39.206580
2691.995923	261941.774802	39.211597
2694.880330	262304.630218	39.216615
2697.635269	262686.126910	39.221632
2700.166651	263050.563269	39.226650
2702.958901	263418.235692	39.231668
2705.492792	263803.426706	39.236685
2708.512839	264173.273906	39.241703
2711.051290	264557.982344	39.246720
2713.908427	264938.423782	39.251738
2716.716577	265325.630575	39.256756
2719.152983	265715.081284	39.261773
2722.121863	266087.885150	39.266791
2724.781569	266498.233398	39.271808
2727.588250	266884.908345	39.276826
2730.405957	267273.741128	39.281844
2733.165380	267683.414098	39.286861
2736.204970	268066.572810	39.291879
2738.846725	268465.163774	39.296896
2741.657160	268866.649668	39.301914
2744.848522	269247.270174	39.306932
2747.848857	269647.786549	39.311949
2750.294565	270037.213517	39.316967
2753.743615	270416.904714	39.321984
2756.269791	270811.603208	39.327002
2758.955815	271190.069207	39.332020
2761.883236	271585.187140	39.337037
2764.902200	271973.736644	39.342055
2767.734078	272376.160749	39.347072
2770.360613	272753.772963	39.352090
2773.376583	273134.651438	39.357108
2775.680767	273537.769084	39.362125
2778.835485	273917.634997	39.367143
2781.836448	274316.552468	39.372160
2784.115070	274710.452878	39.377178
2786.814210	275093.109210	39.382196
2789.511442	275498.146265	39.387213
2792.359313	275888.450876	39.392231
2795.179169	276284.374056	39.397248
2797.640744	276671.208706	39.402266
2801.214498	277031.015781	39.407284
2803.521782	277399.558897	39.412301
2805.948858	277754.415945	39.417319
2808.463575	278119.267974	39.422336
2810.878885	278485.837680	39.427354
2813.919376	278851.063517	39.432372
2816.685982	279237.010950	39.437389
2819.196854	279613.650298	39.442407
2822.056128	280000.217843	39.447424
2824.187030	280389.948950	39.452442
2827.235657	280785.275701	39.457460
2829.774881	281200.040223	39.462477
2832.659490	281602.429209	39.467495
2835.685827	282001.162835	39.472512
2838.258418	282417.597907	39.477530
2841.277488	282831.929721	39.482548
2844.421832	283250.026462	39.487565
2847.532967	283662.209175	39.492583
2850.111383	284081.461761	39.497600
2852.525102	284507.395671	39.502618
2855.705483	284922.665484	39.507636
2858.643708	285346.788106	39.512653
2861.376184	285774.677113	39.517671
2864.592529	286204.673700	39.522688
2867.489496	286630.884504	39.527706
2870.316845	287063.736003	39.532724
2873.444044	287498.266888	39.537741
2876.178109	287929.252236	39.542759
2879.309407	288356.541504	39.547776
2881.963959	288801.103394	39.552794
2885.289956	289227.344511	39.557812
2888.139135	289664.685300	39.562829
2890.941955	290106.605245	39.567847
2894.095590	290538.815919	39.572864
2897.048251	290981.269575	39.577882
2900.207733	291412.995239	39.582900
2903.099600	291860.715340	39.587917
2905.935660	292290.991936	39.592935
2908.796940	292723.245160	39.597952
2911.721716	293157.113287	39.602970
2915.206631	293589.316967	39.607988
2918.413777	294030.327582	39.613005
2921.057573	294464.898104	39.618023
2923.974223	294890.838594	39.623040
2926.835602	295321.689580	39.628058
2929.885230	295764.372636	39.633076
2932.770591	296196.056222	39.638093
2935.607490	296632.979336	39.643111
2938.485033	297066.059323	39.648128
2941.290687	297519.191767	39.653146
2944.503302	297949.168425	39.658164
2947.180784	298393.072719	39.663181
2950.046061	298829.478073	39.668199
2953.164613	299280.752986	39.673216
2956.215963	299712.401940	39.678234
2959.131010	300111.938471	39.683252
2961.789749	300523.935900	39.688269
2964.602076	300923.893122	39.693287
2967.365284	301332.569759	39.698304
2970.000121	301752.848609	39.703322
2972.874863	302158.787486	39.708340
2975.923013	302580.344902	39.713357
2978.437917	303004.627238	39.718375
2981.420402	303438.766108	39.723392
2984.050876	303870.495510	39.728410
2987.103585	304303.731623	39.733428
2990.269161	304756.608681	39.738445
2992.938087	305199.936032	39.743463
2995.991861	305640.660973	39.748480
2998.864299	306106.153211	39.753498
3001.662987	306558.752100	39.758516
3004.572452	307026.013241	39.763533
3007.501081	307493.803054	39.768551
3010.913075	307964.638845	39.773568
3013.830730	308434.865300	39.778586
3017.109903	308907.852126	39.783604
3020.098223	309385.328104	39.788621
3023.075374	309871.058840	39.793639
3026.179012	310337.032083	39.798656
3029.129018	310838.409242	39.803674
3032.352291	311314.570193	39.808692
3035.097437	311793.014546	39.813709
3038.238483	312294.304221	39.818727
3041.391455	312782.661623	39.823744
3044.489484	313278.518206	39.828762
3047.897173	313773.078951	39.833780
3050.780430	314255.986194	39.838797
3053.822652	314758.372142	39.843815
3057.415418	315243.169001	39.848832
3060.367102	315748.155073	39.853850
3063.533005	316231.567055	39.858868
3066.319320	316731.469304	39.863885
3069.502790	317244.309900	39.868903
3073.077377	317725.973600	39.873920
3075.968574	318222.829244	39.878938
3079.255513	318712.863919	39.883956
3082.573563	319214.218353	39.888973
3085.637002	319706.340369	39.893991
3089.153021	320191.505509	39.899008
3091.925022	320685.750926	39.904026
3095.137938	321170.654003	39.909044
3098.467139	321658.888399	39.914061
3101.367762	322146.756158	39.919079
3104.562636	322640.542779	39.924096
3107.763130	323135.976437	39.929114
3110.333346	323609.132954	39.934132
3113.444492	324114.073185	39.939149
3116.316850	324615.187980	39.944167
3120.048636	325104.100805	39.949184
3123.126306	325600.529700	39.954202
3126.022138	326065.163927	39.959220
3129.481127	326504.184152	39.964237
3132.258367	326962.381538	39.969255
3135.403363	327414.981978	39.974272
3138.558849	327866.867085	39.979290
3141.143426	328327.397881	39.984308
3144.495038	328774.116927	39.989325
3147.056522	329255.393090	39.994343
3150.315198	329723.934974	39.999360
3153.355772	330208.049569	40.004378
3155.904490	330685.103154	40.009396
3159.152151	331171.311756	40.014413
3161.939814	331669.321694	40.019431
3165.216554	332163.797330	40.024448
3168.138080	332672.571309	40.029466
3171.308167	333185.796873	40.034484
3174.573743	333695.677134	40.039501
3177.077145	334224.490158	40.044519
3180.852417	334745.632558	40.049536
3184.141435	335271.215380	40.054554
3187.384379	335795.811138	40.059572
3190.854752	336323.058360	40.064589
3193.901750	336852.298158	40.069607
3197.339788	337386.753272	40.074624
3200.320374	337925.212034	40.079642
3203.860364	338447.962393	40.084660
3207.349637	338982.421685	40.089677
3210.451462	339522.117476	40.094695
3214.103562	340054.358428	40.099712
3217.371199	340583.532710	40.104730
3220.549173	341127.519003	40.109748
3224.090408	341651.131305	40.114765
3227.551761	342181.657713	40.119783
3230.868905	342716.721596	40.124800
3233.991767	343256.203772	40.129818
3236.941362	343782.684054	40.134836
3240.332027	344320.387816	40.139853
3243.498041	344865.180168	40.144871
3247.039426	345389.546826	40.149888
3250.424844	345935.614656	40.154906
3253.355171	346480.581470	40.159924
3256.838809	347012.482624	40.164941
3260.022201	347553.565657	40.169959
3263.740794	348094.635002	40.174976
3266.984785	348632.093120	40.179994
3270.193635	349170.795528	40.185012
3273.488663	349710.316784	40.190029
3276.528389	350256.803453	40.195047
3280.092674	350784.314737	40.200064
3283.755488	351324.117197	40.205082
3286.667955	351861.545151	40.210100
3290.310147	352390.170630	40.215117
3293.537343	352935.280307	40.220135
3296.524090	353460.394087	40.225152
3299.943693	353989.368650	40.230170
3303.003599	354499.356806	40.235188
3306.300575	354991.381579	40.240205
3309.141444	355491.723344	40.245223
3312.297382	355983.456240	40.250240
3315.655110	356487.463119	40.255258
3318.423807	357003.868653	40.260276
3321.728305	357508.355927	40.265293
3324.832811	358031.373227	40.270311
3327.743325	358553.755721	40.275328
3330.969673	359092.199956	40.280346
3334.084709	359632.914758	40.285364
3337.688253	360162.480151	40.290381
3340.391814	360721.775888	40.295399
3344.013643	361272.925028	40.300416
3347.509408	361822.945585	40.305434
3350.510069	362391.793659	40.310452
3353.978295	362953.023170	40.315469
3357.302671	363526.222226	40.320487
3360.743494	364088.406710	40.325504
3364.153655	364682.109265	40.330522
3367.590673	365258.517292	40.335540
3371.296630	365830.459700	40.340557
3374.021693	366411.736607	40.345575
3377.803682	367001.390937	40.350592
3381.261191	367591.951555	40.355610
3384.707456	368181.465604	40.360628
3388.366893	368761.802588	40.365645
3391.846186	369366.318117	40.370663
3395.551871	369954.219213	40.375680
3399.104840	370541.705039	40.380698
3402.462705	371126.346285	40.385716
3406.172666	371717.673409	40.390733
3409.375089	372315.568258	40.395751
3413.302386	372904.205434	40.400768
3416.923555	373482.175142	40.405786
3420.186366	374085.820178	40.410804
3423.754669	374664.339909	40.415821
3427.277933	375252.779145	40.420839
3430.600657	375840.886372	40.425856
3433.995269	376425.218699	40.430874
3437.168608	377026.144888	40.435892
3441.158012	377609.401817	40.440909
3443.932854	378201.899448	40.445927
3447.595707	378814.898996	40.450944
3451.386802	379390.347030	40.455962
3454.587070	379988.255680	40.460980
3458.476746	380592.007816	40.465997
3461.634245	381188.331835	40.471015
3465.050537	381777.578727	40.476032
3468.694801	382387.607344	40.481050
3472.041500	382986.359406	40.486068
3475.865271	383580.714187	40.491085
3479.220195	384176.731767	40.496103
3482.725327	384771.118026	40.501120
3486.485814	385341.711568	40.506125
3489.736870	385886.170214	40.511130
3492.842799	386370.629398	40.516135
3495.791094	386811.495491	40.521140
3498.692090	387200.513530	40.526144
3500.947576	387527.633552	40.531149
3502.891246	387823.319058	40.536154
3505.630975	388054.516454	40.541159
3507.478010	388250.736729	40.546164
3508.734746	388394.641339	40.551168
3510.368518	388508.480359	40.556173
3511.405462	388595.637410	40.561178
3512.872755	388629.352383	40.566183
3513.635403	388656.541948	40.571188
3514.431360	388645.253337	40.576192
3515.384737	388620.640869	40.581197
3515.658082	388566.689938	40.586202
3516.606291	388495.671552	40.591207
3516.629035	388413.941398	40.596212
3516.696115	388312.344425	40.601216
3517.188609	388188.124799	40.606221
3517.235734	388064.407435	40.611226
3517.377755	387940.725503	40.616231
3517.034545	387802.879713	40.621236
3517.055754	387663.551772	40.626240
3517.147372	387509.005609	40.631245
3516.647022	387370.191279	40.636250
3516.656597	387223.260176	40.641255
3516.851895	387067.424283	40.646260
3516.612686	386912.037851	40.651264
3516.490489	386753.453564	40.656269
3516.060004	386609.081644	40.661274
3516.213341	386439.237958	40.666279
3515.598637	386293.927582	40.671284
3515.296264	386139.005586	40.676288
3515.240782	385984.679661	40.681293
3514.764332	385835.531102	40.686298
3514.610614	385674.251529	40.691303
3514.301317	385535.501756	40.696308
3513.976936	385399.424047	40.701312
3513.967863	385246.689817	40.706317
3513.584932	385113.544831	40.711322
3513.448482	384982.242281	40.716327
3513.119678	384858.548072	40.721332
3512.567952	384718.765464	40.726336
3512.527770	384592.354493	40.731341
3512.217672	384484.474190	40.736346
3512.135810	384351.202587	40.741351
3511.866001	384236.525064	40.746356
3511.476306	384134.454665	40.751360
3511.526716	384018.377992	40.756365
3511.164729	383914.064645	40.761370
3511.016292	383815.439355	40.766375
3510.342859	383717.532588	40.771380
3510.324136	383609.069635	40.776384
3510.506937	383518.834534	40.781389
3510.074922	383431.697362	40.786394
3510.021377	383339.413780	40.791399
3509.698498	383254.064610	40.796404
3509.552969	383173.112381	40.801408
3509.951223	383086.936740	40.806413
3509.365580	383004.248044	40.811418
3509.247002	382922.197435	40.816423
3508.981476	382862.855425	40.821428
3508.723390	382775.841836	40.826432
3508.937663	382695.314919	40.831437
3508.682714	382635.716557	40.836442
3508.540716	382558.246689	40.841447
3508.414183	382494.558617	40.846452
3507.927852	382427.290465	40.851456
3508.183431	382367.432950	40.856461
3507.681996	382309.805914	40.861466
3507.691083	382246.248582	40.866471
3507.333871	382196.533557	40.871476
3507.615231	382139.240306	40.876480
3507.585524	382084.005330	40.881485
3507.397612	382035.738430	40.886490
3507.169043	381970.234450	40.891495
3507.267226	381934.409708	40.896500
3507.188072	381873.993944	40.901504
3507.395744	381819.865540	40.906509
3507.312167	381792.640289	40.911514
3507.242101	381723.499353	40.916519
3506.813939	381694.878824	40.921524
3506.671885	381650.927799	40.926528
3507.294486	381594.419078	40.931533
3506.991481	381550.874877	40.936538
3506.902939	381508.466647	40.941543
3506.520960	381469.792565	40.946548
3506.854747	381417.576575	40.951552
3506.747623	381374.942237	40.956557
3506.642194	381339.199990	40.961562
3506.582390	381288.572039	40.966567
3506.641086	381253.287000	40.971572
3506.326796	381212.338394	40.976576
3506.605186	381165.217482	40.981581
3506.068108	381129.441543	40.986586
3505.973817	381078.717033	40.991591
3505.985937	381046.516609	40.996596
3505.549450	381018.532727	41.001600
3505.855301	380999.180587	41.006605
3505.419631	380968.068223	41.011610
3505.844205	380931.555111	41.016615
3505.528369	380912.504672	41.021620
3505.294905	380885.327905	41.026624
3505.695812	380871.428885	41.031629
3505.536056	380846.732926	41.036634
3505.486035	380810.294723	41.041639
3505.533985	380782.462992	41.046644
3505.533733	380759.547549	41.051648
3505.712290	380734.391100	41.056653
3505.383568	380724.142642	41.061658
3505.636383	380685.494589	41.066663
3505.537385	380662.086025	41.071668
3505.353671	380633.324327	41.076672
3505.129800	380609.274194	41.081677
3505.238081	380587.791215	41.086682
3505.349007	380569.868529	41.091687
3505.266922	380559.937111	41.096692
3505.295594	380531.040028	41.101696
3505.499227	380500.055129	41.106701
3505.344272	380490.160646	41.111706
3505.436388	380455.327403	41.116711
3505.441645	380439.201728	41.121716
3505.295801	380422.438653	41.126720
3505.233413	380385.188122	41.131725
3504.833336	380372.051389	41.136730
3505.093624	380337.216889	41.141735
3505.030116	380325.629271	41.146740
3505.116657	380305.548435	41.151744
3505.120729	380289.956998	41.156749
3504.946554	380280.803084	41.161754
3505.342306	380255.790028	41.166759
3505.090170	380236.093336	41.171764
3505.059333	380215.369727	41.176768
3505.462407	380200.707104	41.181773
3505.164407	380178.601405	41.186778
3505.130388	380145.669939	41.191783
3505.242562	380130.900672	41.196788
3505.022056	380113.106470	41.201792
3504.831810	380088.567452	41.206797
3504.979079	380069.189048	41.211802
3504.936421	380044.931880	41.216807
3505.316836	380032.434674	41.221812
3505.182476	380001.426505	41.226816
3505.057210	379991.959581	41.231821
3505.207279	379968.969040	41.236826
3505.092083	379944.875881	41.241831
3504.709466	379930.515399	41.246836
3504.968205	379895.502708	41.251840
3504.947496	379889.707188	41.256845
3504.795947	379875.284724	41.261850
3505.098844	379850.311520	41.266855
3505.236675	379842.710535	41.271860
3504.851980	379827.714488	41.276864
3505.174974	379806.349739	41.281869
3504.921007	379780.599756	41.286874
3505.116510	379762.561591	41.291879
3505.114774	379736.848008	41.296884
3505.196676	379721.905331	41.301888
3504.970830	379693.912626	41.306893
3504.579810	379675.254978	41.311898
3504.951679	379659.935793	41.316903
3504.580536	379636.391590	41.321908
3504.540915	379639.068663	41.326912
3504.753970	379608.310472	41.331917
3504.614819	379607.900287	41.336922
3504.415019	379585.855030	41.341927
3504.364574	379588.533817	41.346932
3504.398171	379569.834428	41.351936
3504.711981	379556.075879	41.356941
3504.448234	379540.729954	41.361946
3504.504056	379523.044407	41.366951
3504.849194	379508.492421	41.371956
3504.637374	379498.352330	41.376960
3504.704210	379488.575138	41.381965
3504.529443	379468.967565	41.386970
3504.761883	379447.311721	41.391975
3504.540632	379441.369795	41.396980
3504.599139	379435.383644	41.401984
3504.588977	379406.669906	41.406989
3504.286080	379407.124942	41.411994
3504.238847	379385.386103	41.416999
3504.514356	379377.941306	41.422004
3504.302872	379376.754082	41.427008
3504.334453	379373.722582	41.432013
3504.432425	379361.549591	41.437018
3504.740921	379338.813413	41.442023
3504.505345	379333.763945	41.447028
3504.325639	379315.962929	41.452032
3504.755397	379299.337289	41.457037
3504.445285	379297.478920	41.462042
3504.661214	379274.350386	41.467047
3504.354121	379265.395287	41.472052
3504.188586	379250.720456	41.477056
3504.542465	379242.474772	41.482061
3504.066823	379239.141926	41.487066
3504.181830	379227.017068	41.492071
3504.298562	379222.369715	41.497076
3504.111493	379211.309991	41.502080
3504.217244	379201.857225	41.507085
3504.366981	379200.180505	41.512090
3504.629073	379176.485053	41.517095
3504.458144	379180.073126	41.522100
3504.102200	379170.082907	41.527104
3504.507583	379152.545410	41.532109
3504.613264	379143.830248	41.537114
3504.839395	379131.102797	41.542119
3504.547463	379123.773088	41.547124
3504.189048	379111.850208	41.552128
3504.398923	379090.324908	41.557133
3504.639527	379077.111892	41.562138
3504.343124	379071.512441	41.567143
3504.191871	379051.595725	41.572148
3504.270340	379055.729384	41.577152
3504.236606	379041.287987	41.582157
3504.158575	379027.107935	41.587162
3504.483591	379016.552204	41.592167
3504.294984	379006.560924	41.597172
3504.240121	378979.354591	41.602176
3504.678242	378986.636185	41.607181
3504.305831	378973.214823	41.612186
3504.423514	378955.773589	41.617191
3504.251864	378957.301578	41.622196
3504.240351	378953.971641	41.627200
3504.076861	378943.137026	41.632205
3504.036678	378926.483779	41.637210
3504.166938	378908.277490	41.642215
3504.283215	378916.932586	41.647220
3503.910626	378911.981027	41.652224
3504.386954	378899.213949	41.657229
3504.438041	378901.317166	41.662234
3504.422671	378884.278455	41.667239
3504.317896	378873.409105	41.672244
3504.171628	378871.168727	41.677248
3504.331143	378853.415616	41.682253
3504.061421	378856.586944	41.687258
3504.543928	378834.458838	41.692263
3504.359590	378811.062652	41.697268
3504.006160	378813.662214	41.702272
3504.227913	378791.168346	41.707277
3503.934993	378782.185461	41.712282
3504.340833	378784.766737	41.717287
3504.331643	378782.962513	41.722292
3504.160634	378758.292443	41.727296
3504.245886	378767.283130	41.732301
3504.102718	378758.454610	41.737306
3504.069262	378748.006345	41.742311
3504.231992	378739.256639	41.747316
3503.948926	378731.111537	41.752320
3504.388280	378719.494819	41.757325
3504.430719	378706.948879	41.762330
3504.454025	378700.688396	41.767335
3504.283196	378685.836147	41.772340
3504.318615	378678.251127	41.777344
3504.372872	378660.412828	41.782349
3503.942988	378654.605503	41.787354
3504.355830	378643.425349	41.792359
3504.394780	378638.688483	41.797364
3504.385953	378631.288493	41.802368
3504.329223	378607.541359	41.807373
3504.316072	378592.816758	41.812378
3504.410079	378587.282696	41.817383
3504.485516	378582.133095	41.822388
3504.039359	378577.015077	41.827392
3504.099199	378567.747463	41.832397
3503.972703	378555.101005	41.837402
3504.154558	378532.511557	41.842407
3504.223474	378538.503540	41.847412
3503.927943	378525.909229	41.852416
3504.075199	378521.053487	41.857421
3503.963065	378519.443570	41.862426
3504.332916	378507.176465	41.867431
3503.926584	378500.373426	41.872436
3503.811885	378492.557750	41.877440
3504.464374	378492.276759	41.882445
3503.914848	378479.798891	41.887450
3503.900956	378466.829382	41.892455
3503.984748	378468.571360	41.897460
3504.265543	378472.037219	41.902464
3504.484026	378447.559734	41.907469
3504.093774	378444.772893	41.912474
3504.009473	378435.680644	41.917479
3503.968581	378420.731448	41.922484
3503.896483	378418.377579	41.927488
3504.409631	378417.304690	41.932493
3504.093249	378399.092467	41.937498
3504.071644	378386.454809	41.942503
3504.109842	378391.688616	41.947508
3503.960567	378378.867656	41.952512
3504.204284	378371.656611	41.957517
3504.165991	378366.016257	41.962522
3504.116901	378348.982646	41.967527
3503.835944	378338.904055	41.972532
3503.733620	378336.936486	41.977536
3503.910813	378326.454809	41.982541
3504.026971	378347.903955	41.987546
3503.959475	378319.656320	41.992551
3503.965285	378315.306182	41.997556
3504.021984	378320.257286	42.002560
3504.085873	378313.685104	42.007565
3503.882946	378297.642327	42.012570
3504.182901	378292.889594	42.017575
3504.202352	378288.054028	42.022580
3504.065940	378270.881575	42.027584
3504.270924	378263.702069	42.032589
3504.033765	378262.315388	42.037594
3504.113410	378245.744651	42.042599
3504.331677	378230.423756	42.047604
3503.904200	378238.630818	42.052608
3503.915204	378231.456536	42.057613
3503.982433	378226.130139	42.062618
3503.896229	378205.414219	42.067623
3503.993746	378206.543592	42.072628
3503.925856	378220.518493	42.077632
3504.285480	378180.859106	42.082637
3503.787695	378189.636869	42.087642
3503.878781	378179.067024	42.092647
3504.023206	378180.392465	42.097652
3504.040760	378172.123419	42.102656
3504.215014	378150.959331	42.107661
3503.894983	378157.826788	42.112666
3504.103241	378145.686857	42.117671
3503.834865	378127.899320	42.122676
3503.676290	378135.478883	42.127680
3504.170077	378117.698034	42.132685
3503.839185	378134.715910	42.137690
3503.854566	378106.404151	42.142695
3504.098564	378112.012427	42.147700
3503.887075	378108.942949	42.152704
3504.101767	378114.174328	42.157709
3504.050170	378095.894672	42.162714
3504.314154	378094.555939	42.167719
3504.000386	378088.781045	42.172724
3503.965092	378073.551045	42.177728
3504.452854	378049.132486	42.182733
3504.283373	378059.359067	42.187738
3504.132518	378036.949108	42.192743
3504.612548	378026.139689	42.197748
3504.204263	378014.097182	42.202752
3504.425966	377985.371190	42.207757
3503.996562	377992.713803	42.212762
3504.297447	377982.136175	42.217767
3504.204418	377961.039674	42.222772
3504.088135	377956.886846	42.227776
3504.396889	377950.784603	42.232781
3504.072365	377941.755651	42.237786
3504.042904	377934.714889	42.242791
3504.140371	377929.612591	42.247796
3504.110271	377908.404373	42.252800
3504.252163	377897.800986	42.257805
3504.348223	377900.507598	42.262810
3504.585646	377887.065769	42.267815
3504.258254	377881.750837	42.272820
3504.291966	377857.200454	42.277824
3504.049857	377841.239993	42.282829
3504.054471	377842.485805	42.287834
3504.143795	377828.278866	42.292839
3504.197842	377806.345096	42.297844
3503.754872	377815.953649	42.302848
3504.227769	377802.703486	42.307853
3503.862594	377785.261760	42.312858
3504.239351	377789.017735	42.317863
3503.936345	377770.090912	42.322868
3503.838908	377782.162971	42.327872
3504.114612	377747.298301	42.332877
3503.941822	377756.864157	42.337882
3503.765464	377748.498499	42.342887
3503.841541	377754.362291	42.347892
3503.679763	377728.952488	42.352896
3504.328252	377719.591620	42.357901
3503.827266	377719.976245	42.362906
3503.846603	377717.836800	42.367911
3504.220632	377708.697366	42.372916
3503.927472	377698.188135	42.377920
3504.040189	377687.640175	42.382925
3503.861801	377700.640738	42.387930
3504.068656	377686.211684	42.392935
3504.034247	377673.423208	42.397940
3503.966517	377666.973468	42.402944
3503.899005	377663.347047	42.407949
3503.631751	377653.952877	42.412954
3503.928454	377649.709295	42.417959
3504.052917	377644.068545	42.422964
3503.942348	377645.764978	42.427968
3503.681484	377646.238823	42.432973
3503.671601	377630.979200	42.437978
3504.075060	377614.458752	42.442983
3503.918501	377603.215704	42.447988
3503.844265	377623.652477	42.452992
3503.973271	377609.235701	42.457997
3503.961554	377603.692780	42.463002
3503.825222	377593.336779	42.468007
3504.338915	377589.542167	42.473012
3503.939887	377584.289390	42.478016
3503.974807	377567.369341	42.483021
3503.742377	377563.234832	42.488026
3503.618936	377564.882432	42.493031
3504.064714	377565.600670	42.498036
3503.702949	377561.283121	42.503040
3504.111623	377528.661016	42.508045
3503.724724	377534.674336	42.513050
3503.821885	377533.819800	42.518055
3504.032011	377536.508405	42.523060
3503.601454	377523.528148	42.528064
3503.756387	377512.083218	42.533069
3504.013945	377504.081321	42.538074
3503.892275	377520.074393	42.543079
3504.039058	377503.950576	42.548084
3504.074537	377500.689395	42.553088
3504.212891	377482.201379	42.558093
3503.451326	377490.792072	42.563098
3503.603774	377489.420080	42.568103
3503.800881	377482.190807	42.573108
3503.571981	377462.616229	42.578112
3503.830315	377452.808261	42.583117
3503.922906	377456.354832	42.588122
3504.183619	377456.186640	42.593127
3504.363864	377441.710833	42.598132
3503.849303	377439.961002	42.603136
3504.209591	377425.151498	42.608141
3504.220823	377425.200795	42.613146
3504.019147	377402.849384	42.618151
3504.144124	377394.537759	42.623156
3503.850943	377397.305938	42.628160
3503.985790	377389.806697	42.633165
3503.715956	377367.923885	42.638170
3503.911021	377368.834375	42.643175
3504.036739	377365.075638	42.648180
3504.047786	377365.404758	42.653184
3504.091396	377333.425228	42.658189
3503.917904	377343.423703	42.663194
3503.899312	377331.268514	42.668199
3504.236863	377323.788088	42.673204
3503.857628	377310.621598	42.678208
3503.764760	377300.004291	42.683213
3503.607202	377310.458102	42.688218
3503.781080	377303.105289	42.693223
3504.087434	377309.466898	42.698228
3503.634414	377293.310635	42.703232
3504.039923	377279.358747	42.708237
3503.781950	377284.283417	42.713242
3503.965815	377280.718967	42.718247
3504.023220	377253.697187	42.723252
3503.796395	377259.990474	42.728256
3504.084727	377242.572381	42.733261
3503.719038	377258.705875	42.738266
3503.844015	377250.394220	42.743271
3504.138257	377220.867696	42.748276
3503.663622	377235.568575	42.753280
3503.795723	377224.661326	42.758285
3503.871349	377236.884243	42.763290
3503.854208	377218.115455	42.768295
3503.830683	377215.957322	42.773300
3503.980050	377208.532060	42.778304
3504.175324	377198.403330	42.783309
3503.671053	377209.446131	42.788314
3503.905478	377177.207387	42.793319
3504.038694	377166.503434	42.798324
3503.838733	377184.442148	42.803329
3503.890515	377171.614450	42.808333
3503.789109	377169.519499	42.813338
3503.511992	377158.041023	42.818343
3503.617303	377140.422894	42.823348
3503.785888	377144.873175	42.828353
3504.196428	377146.003967	42.833357
3503.857345	377144.531614	42.838362
3503.996910	377126.730013	42.843367
3503.964844	377121.113933	42.848372
3504.083196	377121.578709	42.853377
3504.328260	377102.234260	42.858381
3503.964469	377084.588520	42.863386
3503.811971	377086.113552	42.868391
3504.015653	377091.626602	42.873396
3503.807192	377073.879994	42.878401
3503.700658	377059.373075	42.883405
3503.983648	377062.660659	42.888410
3503.824853	377055.436699	42.893415
3503.992074	377050.603058	42.898420
3503.950936	377053.687521	42.903425
3504.357046	377036.301592	42.908429
3504.125976	377030.106493	42.913434
3503.976555	377020.032209	42.918439
3503.959542	377002.331613	42.923444
3504.211178	376990.057293	42.928449
3503.981658	376989.712237	42.933453
3503.888488	376976.398670	42.938458
3503.842132	376965.316073	42.943463
3504.015261	376957.836135	42.948468
3503.589591	376958.895634	42.953473
3503.606704	376964.539939	42.958477
3503.743181	376966.553452	42.963482
3503.473834	376953.394909	42.968487
3503.542762	376938.554975	42.973492
3503.432189	376944.041416	42.978497
3503.366967	376941.991604	42.983501
3503.429800	376939.540008	42.988506
3503.635611	376939.304186	42.993511
3503.603041	376940.759393	42.998516
3503.742368	376942.238299	43.003521
3503.666832	376947.617456	43.008525
3503.751223	376958.541832	43.013530
3503.721140	376937.307658	43.018535
3503.775221	376933.611076	43.023540
3503.874032	376923.319474	43.028545
3503.636899	376920.635499	43.033549
3503.692446	376926.070245	43.038554
3503.741803	376924.485606	43.043559
3503.944121	376904.944331	43.048564
3503.695809	376897.124027	43.053569
3504.089219	376903.395630	43.058573
3503.673952	376893.108978	43.063578
3503.558276	376900.020654	43.068583
3503.518705	376908.929750	43.073588
3503.401763	376897.578496	43.078593
3503.778657	376881.570668	43.083597
3503.767026	376881.572708	43.088602
3503.720586	376870.617279	43.093607
3504.104488	376870.480484	43.098612
3503.839858	376874.770353	43.103617
3503.870094	376861.793345	43.108621
3504.113735	376862.263754	43.113626
3503.756736	376848.203331	43.118631
3504.068319	376857.362161	43.123636
3503.796830	376843.033857	43.128641
3503.724600	376821.958901	43.133645
3503.805564	376829.246483	43.138650
3503.619371	376823.171439	43.143655
3504.100343	376812.819396	43.148660
3503.833406	376825.020283	43.153665
3504.017549	376800.852448	43.158669
3504.033794	376797.721432	43.163674
3503.606082	376785.478134	43.168679
3504.024286	376782.563371	43.173684
3503.601152	376779.781610	43.178689
3503.927247	376765.689481	43.183693
3503.518633	376766.135820	43.188698
3503.365921	376770.509752	43.193703
3504.001031	376773.843441	43.198708
3503.580335	376769.891228	43.203713
3503.751273	376773.298293	43.208717
3503.586297	376776.071684	43.213722
3503.750031	376753.814762	43.218727
3503.499044	376748.156929	43.223732
3503.454220	376749.257973	43.228737
3503.719029	376733.420423	43.233741
3503.944576	376741.753485	43.238746
3503.872407	376746.445359	43.243751
3503.633012	376740.251532	43.248756
3503.607105	376722.781144	43.253761
3503.584062	376708.540698	43.258765
3503.756155	376717.136578	43.263770
3503.811267	376710.616391	43.268775
3503.959285	376715.324333	43.273780
3503.792179	376727.000744	43.278785
3503.905888	376699.181166	43.283789
3504.108960	376694.265507	43.288794
3503.377613	376686.089104	43.293799
3503.715295	376687.867334	43.298804
3503.755894	376704.598167	43.303809
3503.832762	376690.341920	43.308813
3503.667257	376676.887071	43.313818
3503.412370	376665.786483	43.318823
3503.645679	376667.403160	43.323828
3503.471813	376669.770983	43.328833
3503.641707	376675.391177	43.333837
3503.852373	376673.475792	43.338842
3503.668025	376674.064734	43.343847
3503.865121	376668.743035	43.348852
3503.660489	376648.350262	43.353857
3503.585525	376640.248141	43.358861
3503.537120	376638.577200	43.363866
3503.648975	376639.424553	43.368871
3503.850378	376631.990958	43.373876
3503.424633	376656.502725	43.378881
3503.731363	376648.416576	43.383885
3503.612614	376638.540837	43.388890
3503.216428	376628.988753	43.393895
3503.934195	376607.992291	43.398900
3503.840424	376619.555395	43.403905
3503.679875	376607.422426	43.408909
3503.594965	376615.651975	43.413914
3503.651859	376615.261638	43.418919
3503.653990	376632.252944	43.423924
3503.526426	376620.598055	43.428929
3503.598538	376595.888209	43.433933
3503.771827	376592.579732	43.438938
3503.811401	376595.727780	43.443943
3503.764583	376589.757850	43.448948
3503.737051	376605.024188	43.453953
3503.590139	376593.041677	43.458957
3503.701606	376603.936433	43.463962
3503.651030	376584.740216	43.468967
3503.957291	376571.058136	43.473972
3503.562906	376573.282770	43.478977
3503.672370	376575.860172	43.483981
3503.887649	376567.584973	43.488986
3503.383877	376575.982490	43.493991
3503.486448	376563.146569	43.498996
3503.509555	376556.555108	43.504001
3503.574501	376545.225873	43.509005
3503.538245	376544.697642	43.514010
3503.257821	376547.692789	43.519015
3503.625982	376532.932584	43.524020
3503.601536	376556.134593	43.529025
3503.528154	376545.005279	43.534029
3503.665260	376559.940372	43.539034
3504.014952	376554.874336	43.544039
3503.708139	376560.010306	43.549044
3503.503905	376530.816438	43.554049
3503.762122	376530.012730	43.559053
3503.770164	376531.741331	43.564058
3503.644317	376531.990354	43.569063
3503.415388	376524.446713	43.574068
3503.530539	376522.190312	43.579073
3504.069984	376525.411962	43.584077
3504.052373	376510.509242	43.589082
3503.514982	376494.162502	43.594087
3503.795521	376494.856010	43.599092
3504.027201	376502.094389	43.604097
3503.875048	376492.376513	43.609101
3503.378792	376487.495071	43.614106
3503.810071	376480.533836	43.619111
3503.899243	376469.709478	43.624116
3503.667404	376473.510914	43.629121
3503.688119	376481.265938	43.634125
3503.804491	376472.116081	43.639130
3503.668758	376462.115802	43.644135
3503.973282	376452.325724	43.649140
3503.648646	376434.012160	43.654145
3503.843792	376444.257821	43.659149
3503.461320	376436.000780	43.664154
3503.499559	376445.584461	43.669159
3503.710362	376442.829643	43.674164
3503.590396	376451.827859	43.679169
3503.746416	376421.076214	43.684173
3503.819364	376420.327228	43.689178
3503.515735	376421.901613	43.694183
3503.721898	376417.977452	43.699188
3503.763250	376424.737203	43.704193
3503.886697	376406.759776	43.709197
3503.620051	376402.121826	43.714202
3503.550901	376402.870616	43.719207
3503.736268	376386.307831	43.724212
3503.645781	376400.464995	43.729217
3503.570677	376384.375805	43.734221
3503.669876	376400.614208	43.739226
3503.849098	376396.516248	43.744231
3503.981026	376395.961429	43.749236
3503.581301	376384.832787	43.754241
3503.974564	376371.772797	43.759245
3504.031084	376378.886269	43.764250
3503.505923	376370.499152	43.769255
3503.986576	376366.302665	43.774260
3503.646327	376359.030955	43.779265
3503.412899	376358.304964	43.784269
3503.311715	376348.935106	43.789274
3503.535586	376331.425063	43.794279
3503.853148	376334.045893	43.799284
3503.636682	376358.702813	43.804289
3503.839875	376352.973126	43.809293
3503.699616	376348.569555	43.814298
3503.690312	376343.153260	43.819303
3503.798981	376320.446947	43.824308
3503.915134	376314.781887	43.829313
3503.908284	376311.323809	43.834317
3503.615489	376310.988749	43.839322
3503.702476	376316.087934	43.844327
3503.788854	376289.315289	43.849332
3503.490593	376289.693315	43.854337
3503.667603	376275.700892	43.859341
3503.604253	376287.844322	43.864346
3503.748220	376284.184345	43.869351
3504.100189	376292.065095	43.874356
3503.775609	376285.019823	43.879361
3503.490843	376271.888929	43.884365
3503.492637	376274.254442	43.889370
3503.658805	376254.616821	43.894375
3503.826227	376264.612545	43.899380
3503.585053	376261.115195	43.904385
3503.994085	376269.571969	43.909389
3503.794305	376244.981199	43.914394
3503.529104	376241.309591	43.919399
3503.828644	376238.438985	43.924404
3503.830338	376240.957135	43.929409
3504.032431	376226.172198	43.934413
3503.544638	376245.047111	43.939418
3504.156290	376222.744524	43.944423
3503.990448	376200.971818	43.949428
3503.714358	376206.230159	43.954433
3503.942892	376210.035152	43.959437
3503.762616	376200.041849	43.964442
3503.249138	376177.739045	43.969447
3503.984180	376182.913856	43.974452
3504.104406	376172.338875	43.979457
3503.986482	376170.042989	43.984461
3503.893842	376163.495198	43.989466
3503.445426	376146.676393	43.994471
3503.769349	376127.675122	43.999476
3503.429791	376134.495138	44.004481
3503.551128	376139.894153	44.009485
3503.819519	376126.828388	44.014490
3503.724808	376139.816227	44.019495
3503.534115	376131.732299	44.024500
3503.705099	376138.853155	44.029505
3503.574193	376113.971615	44.034509
3503.385869	376114.281390	44.039514
3503.442699	376110.202749	44.044519
3503.749303	376103.566398	44.049524
3503.494668	376116.681273	44.054529
3503.458699	376106.258149	44.059533
3503.695307	376113.597565	44.064538
3503.456269	376112.541780	44.069543
3503.840114	376122.579636	44.074548
3503.723087	376114.509496	44.079553
3503.894778	376089.656415	44.084557
3503.725356	376083.400551	44.089562
3503.418259	376082.660764	44.094567
3503.951138	376071.231987	44.099572
3503.536544	376087.678921	44.104577
3503.728100	376084.443825	44.109581
3503.773556	376080.570473	44.114586
3503.786976	376064.060174	44.119591
3503.901609	376049.975788	44.124596
3503.858168	376054.027284	44.129601
3503.851341	376055.580200	44.134605
3503.494232	376056.196461	44.139610
3503.637756	376051.315573	44.144615
3503.803031	376024.199604	44.149620
3503.542294	376032.685997	44.154625
3503.588535	376031.407055	44.159629
3503.617957	376027.230993	44.164634
3503.665697	376016.743739	44.169639
3503.838135	376022.923229	44.174644
3503.735573	376028.255907	44.179649
3503.612062	376012.352277	44.184653
3503.793615	375995.891682	44.189658
3503.540453	375992.269021	44.194663
3503.808049	375990.497225	44.199668
3503.711758	376000.204026	44.204673
3503.401687	376001.448769	44.209677
3503.774455	375996.735129	44.214682
3503.626993	375984.956017	44.219687
3503.729285	375968.126390	44.224692
3503.833204	375964.599898	44.229697
3504.172792	375971.058213	44.234701
3503.974506	375971.954608	44.239706
3503.703959	375949.893078	44.244711
3503.935608	375938.257516	44.249716
3503.862228	375939.108730	44.254721
3503.781443	375932.889704	44.259725
3503.905003	375936.813065	44.264730
3503.816479	375932.859132	44.269735
3503.849307	375917.846472	44.274740
3503.476998	375915.005742	44.279745
3503.645291	375911.698000	44.284749
3503.699613	375906.373335	44.289754
3503.593123	375914.504691	44.294759
3503.877061	375899.325144	44.299764
3503.682257	375896.837903	44.304769
3503.762302	375873.983243	44.309773
3503.924220	375873.398240	44.314778
3504.071487	375872.306817	44.319783
3504.082861	375864.572443	44.324788
3503.497898	375863.545899	44.329793
3504.090476	375842.390773	44.334797
3503.612217	375853.760509	44.339802
3503.687941	375850.696327	44.344807
3503.929899	375844.884130	44.349812
3503.686453	375836.630424	44.354817
3503.480740	375828.599683	44.359821
3503.249986	375816.884563	44.364826
3503.481108	375822.444324	44.369831
3503.428598	375813.117521	44.374836
3503.334741	375822.289807	44.379841
3503.388371	375818.644069	44.384845
3503.529373	375821.369154	44.389850
3503.326004	375826.183622	44.394855
3504.010856	375819.105879	44.399860
3503.427477	375823.878673	44.404865
3503.592499	375824.895696	44.409869
3503.945132	375829.876637	44.414874
3503.701236	375809.693140	44.419879
3503.736635	375793.306440	44.424884
3503.474840	375806.549732	44.429889
3503.571217	375787.329905	44.434893
3503.645384	375801.130571	44.439898
3503.526387	375800.462790	44.444903
3503.548882	375799.213032	44.449908
3503.352128	375803.466847	44.454913
3503.356033	375809.571265	44.459917
3503.300062	375821.255806	44.464922
3503.367398	375808.196284	44.469927
3503.821976	375794.312437	44.474932
3503.810159	375782.613570	44.479937
3503.648051	375763.383720	44.484941
3503.713292	375771.157278	44.489946
3503.344648	375780.423887	44.494951
3503.613385	375773.768031	44.499956
3503.538692	375777.239449	44.504961
3503.332090	375788.846064	44.509965
3503.387526	375790.033032	44.514970
3503.266743	375783.871181	44.519975
3503.457428	375784.477159	44.524980
3503.220514	375794.079055	44.529985
3503.493806	375791.873925	44.534989
3503.769839	375788.040404	44.539994
3503.446545	375783.462212	44.544999
3503.798082	375757.308655	44.550004
3503.441994	375763.317368	44.555009
3503.322779	375753.517796	44.560013
3503.532577	375754.807548	44.565018
3503.461926	375752.783971	44.570023
3503.958950	375757.207922	44.575028
3503.525771	375755.775828	44.580033
3503.819486	375749.116020	44.585037
3503.626911	375753.343743	44.590042
3503.278409	375748.489726	44.595047
3503.419772	375730.483729	44.600052
3503.337647	375731.972251	44.605057
3503.454328	375733.073228	44.610061
3503.493526	375734.898687	44.615066
3503.460912	375735.158412	44.620071
3503.731832	375728.349583	44.625076
3503.481830	375743.905784	44.630081
3503.987482	375729.581415	44.635085
3503.556344	375726.317544	44.640090
3503.555351	375736.060217	44.645095
3503.934210	375722.747926	44.650100
3504.236078	375711.304693	44.655105
3503.889758	375718.278469	44.660109
3504.002591	375728.995187	44.665114
3503.722608	375730.693045	44.670119
3503.879859	375703.120266	44.675124
3503.668171	375712.972563	44.680129
3503.994688	375697.608152	44.685133
3503.805131	375701.046860	44.690138
3503.853916	375706.635461	44.695143
3504.005285	375686.084176	44.700148
3503.690299	375669.549321	44.705153
3503.937680	375670.655076	44.710157
3503.764346	375667.172387	44.715162
3503.611128	375669.791373	44.720167
3503.690290	375647.013036	44.725172
3503.500528	375636.257986	44.730177
3503.682419	375643.250021	44.735181
3504.175103	375637.220100	44.740186
3504.003840	375635.644850	44.745191
3503.850664	375630.632757	44.750196
3503.432971	375613.936057	44.755201
3503.869485	375608.500061	44.760205
3503.662767	375607.668086	44.765210
3503.604887	375605.845978	44.770215
3503.842741	375607.512853	44.775220
3503.638630	375614.082612	44.780225
3503.506863	375606.904993	44.785229
3503.924472	375584.073117	44.790234
3503.693049	375579.047951	44.795239
3503.862829	375577.902087	44.800244
3503.627823	375576.413222	44.805249
3503.874001	375566.097978	44.810253
3503.989085	375567.097465	44.815258
3503.730886	375552.817474	44.820263
3504.061768	375533.992884	44.825268
3503.475344	375544.642133	44.830273
3503.261689	375530.355093	44.835277
3503.837704	375529.246758	44.840282
3503.723508	375542.746608	44.845287
3503.547735	375513.318573	44.850292
3503.567015	375506.218806	44.855297
3503.565514	375499.071449	44.860301
3503.627453	375501.758181	44.865306
3503.337375	375507.400377	44.870311
3503.921989	375498.939390	44.875316
3503.651636	375511.904323	44.880321
3503.673210	375502.591174	44.885325
3503.926480	375501.711917	44.890330
3503.872807	375479.641284	44.895335
3503.879994	375479.513164	44.900340
3503.648702	375471.766203	44.905345
3503.811058	375476.192216	44.910349
3504.078269	375486.986342	44.915354
3503.454129	375463.962964	44.920359
3503.636722	375445.924886	44.925364
3503.407021	375449.013843	44.930369
3503.159752	375445.924379	44.935373
3503.495947	375426.615596	44.940378
3503.544146	375420.477850	44.945383
3503.620439	375432.319653	44.950388
3503.271117	375434.384603	44.955393
3503.596185	375424.998022	44.960397
3503.685361	375428.672498	44.965402
3503.327654	375438.395322	44.970407
3503.643006	375436.794012	44.975412
3503.446175	375436.749018	44.980417
3503.573905	375417.956490	44.985421
3503.913112	375417.419764	44.990426
3503.628449	375404.135950	44.995431
3503.738646	375397.403347	45.000436
3503.645985	375400.979385	45.005441
3503.691171	375400.667199	45.010445
3503.608821	375400.604107	45.015450
3503.632562	375399.990066	45.020455
3503.689848	375379.453499	45.025460
3503.678473	375378.438015	45.030465
3503.577048	375370.695942	45.035469
3503.556323	375371.233599	45.040474
3503.287377	375385.851759	45.045479
3503.573011	375376.929269	45.050484
3503.264022	375387.890820	45.055489
3503.484995	375385.490442	45.060493
3503.712536	375375.661400	45.065498
3503.696532	375389.858017	45.070503
3503.537613	375375.257025	45.075508
3503.242480	375358.286474	45.080513
3503.449525	375351.131561	45.085517
3503.221542	375356.662214	45.090522
3503.008820	375354.839135	45.095527
3503.585018	375368.586024	45.100532
3503.268007	375366.474187	45.105537
3503.803576	375371.146458	45.110541
3503.515562	375361.678722	45.115546
3503.277508	375363.548025	45.120551
3503.479957	375356.419276	45.125556
3503.660389	375353.007822	45.130561
3503.709960	375354.882531	45.135565
3503.778653	375361.841635	45.140570
3503.920341	375366.677921	45.145575
3504.068510	375349.713600	45.150580
3503.604240	375330.429563	45.155585
3503.371614	375317.137494	45.160589
3503.733089	375321.964478	45.165594
3503.570983	375329.850371	45.170599
3503.529087	375331.561482	45.175604
3503.782081	375332.361114	45.180609
3503.775796	375329.309856	45.185613
3503.555810	375312.632652	45.190618
3503.457212	375305.653233	45.195623
3503.933232	375283.244387	45.200628
3503.656153	375308.293084	45.205633
3503.715214	375298.312598	45.210637
3504.074783	375295.305251	45.215642
3503.588650	375288.336218	45.220647
3503.895864	375261.222738	45.225652
3503.720482	375263.997876	45.230657
3503.786752	375263.275361	45.235661
3503.969654	375264.950938	45.240666
3503.833005	375261.386104	45.245671
3503.953408	375230.359377	45.250676
3503.685249	375238.109431	45.255681
3503.649273	375232.112149	45.260685
3503.781657	375223.926092	45.265690
3503.284618	375235.375280	45.270695
3503.327935	375229.696146	45.275700
3503.666987	375233.178515	45.280705
3503.462762	375221.001160	45.285709
3503.545340	375210.075759	45.290714
3503.155035	375206.754516	45.295719
3503.652664	375185.029004	45.300724
3503.654941	375196.755391	45.305729
3503.620507	375201.034483	45.310733
3503.952054	375197.599127	45.315738
3503.512131	375199.449476	45.320743
3503.743091	375185.702521	45.325748
3503.678045	375197.261489	45.330753
3503.648226	375173.737000	45.335757
3503.698657	375167.369928	45.340762
3503.379292	375169.455592	45.345767
3503.690759	375165.540101	45.350772
3503.414300	375180.820890	45.355777
3503.368182	375171.899924	45.360781
3503.522339	375177.395629	45.365786
3503.449923	375178.679138	45.370791
3503.299922	375177.685564	45.375796
3503.567368	375181.815188	45.380801
3503.859179	375176.147638	45.385805
3503.647098	375163.259266	45.390810
3503.363735	375153.053066	45.395815
3503.354446	375141.938671	45.400820
3503.116434	375136.176812	45.405825
3503.483884	375156.545012	45.410829
3503.535179	375169.052212	45.415834
3503.443368	375169.448485	45.420839
3503.748593	375168.052263	45.425844
3503.432814	375184.255006	45.430849
3503.429618	375176.522805	45.435853
3503.682557	375162.899554	45.440858
3503.509248	375161.273734	45.445863
3503.866392	375160.047365	45.450868
3503.717441	375165.031369	45.455873
3503.365175	375148.222386	45.460877
3503.603392	375122.849453	45.465882
3503.597555	375122.901451	45.470887
3503.598656	375118.119279	45.475892
3503.380741	375124.793047	45.480897
3503.389998	375114.591454	45.485901
3503.834653	375121.414854	45.490906
3503.389567	375126.674611	45.495911
3503.596469	375127.303473	45.500916
3503.605332	375122.113078	45.505921
3503.433170	375120.639698	45.510925
3503.539154	375110.829809	45.515930
3503.429630	375095.177981	45.520935
3503.273463	375089.021617	45.525940
3503.367437	375104.345625	45.530945
3503.436827	375096.372998	45.535949
3503.612708	375084.720571	45.540954
3503.400349	375092.436394	45.545959
3503.640109	375092.475005	45.550964
3503.411441	375101.567016	45.555969
3503.461447	375090.799355	45.560973
3503.706528	375104.217119	45.565978
3503.724741	375100.627789	45.570983
3503.748682	375102.862684	45.575988
3503.647350	375087.413056	45.580993
3503.701711	375071.938809	45.585997
3503.953198	375068.083665	45.591002
3503.495610	375072.734911	45.596007
3503.568581	375070.688596	45.601012
3503.568924	375082.822317	45.606017
3503.236593	375068.604750	45.611021
3503.475176	375076.732598	45.616026
3503.724773	375089.615469	45.621031
3503.594576	375072.491540	45.626036
3503.415510	375063.820503	45.631041
3503.572273	375064.737102	45.636045
3503.667201	375072.938534	45.641050
3503.762952	375064.758236	45.646055
3503.910331	375070.433087	45.651060
3503.945138	375068.189307	45.656065
3504.088687	375067.683508	45.661069
3503.763990	375051.989366	45.666074
3503.579342	375056.190471	45.671079
3503.994580	375049.562213	45.676084
3503.423533	375050.161433	45.681089
3503.363051	375055.436712	45.686093
3503.740642	375045.304060	45.691098
3503.686235	375038.851792	45.696103
3503.713327	375012.977983	45.701108
3503.957240	375014.923735	45.706113
3503.682231	375008.455461	45.711117
3503.837082	374999.655312	45.716122
3503.648944	375014.820452	45.721127
3504.108553	375000.248733	45.726132
3503.729906	374981.154493	45.731137
3503.618457	374976.619032	45.736141
3503.682615	374972.157559	45.741146
3503.469737	374974.353586	45.746151
3503.600301	374973.341092	45.751156
3503.670951	374975.441423	45.756161
3503.457441	374965.351320	45.761165
3503.411632	374957.854749	45.766170
3503.660028	374946.699566	45.771175
3503.787427	374936.606438	45.776180
3503.571910	374940.278250	45.781185
3503.520108	374938.709525	45.786189
3503.929156	374949.659434	45.791194
3503.789741	374940.193545	45.796199
3503.603275	374920.661899	45.801204
3503.681161	374918.106051	45.806209
3504.063364	374911.075995	45.811213
3503.834265	374907.576620	45.816218
3503.247524	374909.882626	45.821223
3503.529210	374910.092671	45.826228
3503.545431	374911.413052	45.831233
3503.328558	374913.355339	45.836237
3503.794353	374915.266021	45.841242
3503.476128	374888.505539	45.846247
3503.674143	374876.111869	45.851252
3503.182962	374873.010045	45.856257
3503.335774	374871.714220	45.861261
3503.646484	374868.943502	45.866266
3503.541324	374874.429366	45.871271
3503.756114	374870.045820	45.876276
3503.802287	374872.022838	45.881281
3503.605085	374863.710749	45.886285
3504.183683	374846.703613	45.891290
3503.568048	374834.133306	45.896295
3503.840763	374806.312731	45.901300
3503.694034	374819.283778	45.906305
3504.017975	374817.910024	45.911309
3503.562410	374811.928135	45.916314
3503.327999	374799.450177	45.921319
3503.467407	374788.820929	45.926324
3503.441401	374786.637621	45.931329
3503.581265	374777.839794	45.936333
3503.855024	374772.403979	45.941338
3503.429439	374783.434999	45.946343
3503.435552	374778.626557	45.951348
3503.433234	374780.916495	45.956353
3503.552134	374784.331955	45.961357
3503.625460	374784.269690	45.966362
3503.154994	374796.452486	45.971367
3503.619718	374777.911639	45.976372
3503.382247	374788.989232	45.981377
3503.335457	374790.548514	45.986381
3503.710607	374791.049034	45.991386
3503.646508	374787.930564	45.996391
3503.261572	374765.123350	46.001396
3503.374001	374776.450882	46.006401
3503.499165	374764.068695	46.011405
3503.260099	374759.273572	46.016410
3503.160671	374761.120988	46.021415
3503.500705	374764.374306	46.026420
3503.595054	374765.885840	46.031425
3503.412021	374770.163030	46.036429
3503.218929	374765.716764	46.041434
3503.341509	374762.924905	46.046439
3503.379172	374762.028842	46.051444
3503.226051	374774.593914	46.056449
3503.470675	374767.890832	46.061453
3503.680942	374765.314048	46.066458
3503.178046	374773.024985	46.071463
3503.438392	374768.990350	46.076468
3503.241614	374777.695830	46.081473
3503.308503	374785.494753	46.086477
3503.439416	374784.583949	46.091482
3503.444509	374774.382929	46.096487
3503.619620	374784.708490	46.101492
3503.384564	374774.469121	46.106497
3503.516438	374783.453332	46.111501
3503.679326	374772.565993	46.116506
3503.150674	374779.568752	46.121511
3503.409880	374782.936595	46.126516
3503.689748	374780.857558	46.131521
3503.374232	374776.481521	46.136525
3503.484972	374752.527570	46.141530
3503.400154	374756.204174	46.146535
3503.671704	374746.546087	46.151540
3503.511080	374754.711669	46.156545
3503.607362	374758.970143	46.161549
3503.617769	374751.439211	46.166554
3503.489006	374752.324641	46.171559
3503.320505	374751.613794	46.176564
3503.603984	374752.891930	46.181569
3503.359809	374765.929273	46.186573
3503.579945	374745.875392	46.191578
3503.469934	374755.559222	46.196583
3503.556314	374749.593401	46.201588
3503.788551	374757.874940	46.206593
3503.412993	374731.581293	46.211597
3503.737657	374719.650867	46.216602
3503.437990	374719.011629	46.221607
3503.360579	374720.295942	46.226612
3503.588386	374719.522444	46.231617
3503.407798	374718.203007	46.236621
3503.531458	374721.973845	46.241626
3503.416862	374726.621784	46.246631
3503.428592	374720.871260	46.251636
3503.556372	374720.291637	46.256641
3503.617341	374735.799062	46.261645
3503.712743	374724.362755	46.266650
3503.355184	374707.376364	46.271655
3503.690519	374690.000619	46.276660
3503.741059	374694.190019	46.281665
3503.677029	374696.642342	46.286669
3503.830792	374685.705548	46.291674
3503.569593	374693.632666	46.296679
3503.506652	374688.758817	46.301684
3503.609887	374694.466137	46.306689
3503.676295	374689.749903	46.311693
3503.706647	374667.767298	46.316698
3503.493190	374660.119112	46.321703
3503.370515	374653.041637	46.326708
3503.621901	374664.474421	46.331713
3503.725802	374660.973258	46.336717
3503.678692	374663.015908	46.341722
3503.416821	374663.133820	46.346727
3503.552608	374659.881990	46.351732
3503.572466	374668.934809	46.356737
3503.653471	374665.437265	46.361741
3503.512588	374632.340076	46.366746
3503.520411	374640.707990	46.371751
3503.526348	374625.444730	46.376756
3503.366891	374621.120319	46.381761
3503.437412	374634.769332	46.386765
3503.443381	374625.763701	46.391770
3503.143335	374624.437707	46.396775
3503.294724	374633.495179	46.401780
3503.415121	374637.164790	46.406785
3503.431085	374642.656975	46.411789
3503.535562	374628.192140	46.416794
3503.572415	374650.596983	46.421799
3503.232257	374636.889253	46.426804
3503.066477	374644.038171	46.431809
3503.390282	374646.022187	46.436813
3503.666259	374639.746566	46.441818
3503.515193	374647.936096	46.446823
3503.825928	374637.559537	46.451828
3503.894457	374637.828718	46.456833
3503.216229	374628.651435	46.461837
3503.891797	374609.771931	46.466842
3503.427197	374599.823181	46.471847
3503.624367	374595.645891	46.476852
3503.564863	374613.945101	46.481857
3503.261180	374616.867753	46.486861
3503.506304	374616.345891	46.491866
3503.477488	374613.374454	46.496871
3504.029073	374612.066457	46.501876
3503.739984	374613.689487	46.506881
3503.549902	374597.744953	46.511885
3503.298090	374588.296750	46.516890
3503.600865	374577.997748	46.521895
3503.488518	374582.390971	46.526900
3503.661557	374593.963348	46.531905
3503.759051	374580.618853	46.536909
3503.721637	374578.691713	46.541914
3503.729423	374587.746459	46.546919
3503.670115	374582.414146	46.551924
3503.706122	374564.475165	46.556929
3503.490291	374564.840174	46.561933
3504.056143	374548.852433	46.566938
3503.794926	374563.113539	46.571943
3503.941844	374555.611866	46.576948
3503.636386	374554.286726	46.581953
3503.553688	374529.523783	46.586957
3503.706841	374514.466147	46.591962
3503.371925	374525.610091	46.596967
3503.714304	374517.110882	46.601972
3503.870693	374525.531647	46.606977
3503.419728	374522.041873	46.611981
3503.821172	374522.436490	46.616986
3503.558115	374523.088779	46.621991
3503.194713	374502.974402	46.626996
3503.432907	374517.996016	46.632001
3503.365024	374500.429557	46.637005
3503.460689	374495.530612	46.642010
3503.386794	374490.226031	46.647015
3503.335206	374495.271038	46.652020
3503.285881	374491.209017	46.657025
3503.476003	374493.926426	46.662029
3503.582084	374499.735074	46.667034
3503.309526	374490.188378	46.672039
3503.398363	374503.834539	46.677044
3503.601977	374508.813763	46.682049
3503.607836	374517.003950	46.687053
3503.771595	374495.966792	46.692058
3503.491679	374510.179997	46.697063
3503.526148	374499.618139	46.702068
3503.981019	374495.374662	46.707073
3503.342741	374491.889060	46.712077
3503.730941	374468.832273	46.717082
3503.373423	374471.966947	46.722087
3503.461069	374465.975447	46.727092
3503.157454	374468.796348	46.732097
3503.280095	374464.020323	46.737101
3503.647606	374469.787647	46.742106
3503.298739	374477.474290	46.747111
3503.613615	374470.912680	46.752116
3503.424711	374473.995260	46.757121
3503.235689	374468.429062	46.762125
3503.510931	374474.617974	46.767130
3503.520092	374472.759780	46.772135
3503.598768	374480.989338	46.777140
3503.687907	374475.887921	46.782145
3503.705345	374482.931590	46.787149
3503.961028	374463.889458	46.792154
3503.655625	374455.543515	46.797159
3503.734656	374450.621757	46.802164
3503.765014	374430.521409	46.807169
3503.518148	374451.419515	46.812173
3503.534711	374450.959221	46.817178
3503.836531	374450.937147	46.822183
3503.747402	374420.782373	46.827188
3503.491565	374410.495323	46.832193
3503.504102	374415.504764	46.837197
3503.688647	374405.860351	46.842202
3503.085608	374413.943313	46.847207
3503.302717	374402.258737	46.852212
3503.657839	374414.183946	46.857217
3503.377704	374401.611344	46.862221
3503.384325	374425.674538	46.867226
3503.374944	374422.267575	46.872231
3503.315950	374408.260945	46.877236
3503.270059	374412.872620	46.882241
3503.265775	374424.447639	46.887245
3503.484881	374419.198481	46.892250
3503.355731	374423.823317	46.897255
3503.302241	374417.243618	46.902260
3503.445156	374429.049743	46.907265
3503.493669	374429.372965	46.912269
3503.658527	374423.699943	46.917274
3503.440677	374427.753735	46.922279
3503.670999	374423.800125	46.927284
3503.608369	374407.733618	46.932289
3503.325155	374397.934209	46.937293
3503.358430	374398.641405	46.942298
3503.256620	374394.638547	46.947303
3503.454539	374384.279759	46.952308
3503.752610	374396.875371	46.957313
3503.381744	374398.791151	46.962317
3503.565130	374390.902118	46.967322
3503.391325	374400.748741	46.972327
3503.573750	374401.254296	46.977332
3503.542821	374407.160928	46.982337
3503.439576	374406.592384	46.987341
3503.768976	374402.623111	46.992346
3503.209483	374407.163353	46.997351
3503.617025	374397.687186	47.002356
3503.651928	374377.636970	47.007361
3503.894797	374369.178900	47.012365
3503.885671	374371.062934	47.017370
3503.487719	374371.761987	47.022375
3503.868037	374365.062827	47.027380
3504.160933	374367.840311	47.032385
3503.585383	374348.776903	47.037389
3503.809569	374325.110021	47.042394
3503.836843	374333.017044	47.047399
3503.600824	374337.480720	47.052404
3504.002588	374331.083416	47.057409
3503.461497	374314.049562	47.062413
3503.570346	374288.543937	47.067418
3503.688723	374283.921192	47.072423
3503.601234	374282.815962	47.077428
3503.845772	374292.011411	47.082433
3503.413010	374294.369422	47.087437
3503.730665	374288.010845	47.092442
3503.564266	374286.638275	47.097447
3503.567036	374293.200979	47.102452
3503.367084	374264.462685	47.107457
3503.375426	374260.060834	47.112461
3503.491838	374261.568899	47.117466
3503.185920	374268.511096	47.122471
3503.548322	374264.358527	47.127476
3503.709173	374251.512664	47.132481
3503.472828	374276.021360	47.137485
3503.367920	374265.990229	47.142490
3503.309459	374273.249435	47.147495
3503.340022	374270.497527	47.152500
3503.212971	374259.961140	47.157505
3503.155990	374270.654211	47.162509
3503.387972	374270.490551	47.167514
3503.342850	374274.567928	47.172519
3503.556110	374269.345113	47.177524
3503.749727	374272.443551	47.182529
3503.648471	374267.601147	47.187533
3504.007429	374269.299809	47.192538
3503.699685	374268.916217	47.197543
3503.583399	374247.745139	47.202548
3503.704215	374247.624490	47.207553
3504.014813	374231.778729	47.212557
3503.948082	374228.864134	47.217562
3503.393498	374246.147947	47.222567
3503.650820	374234.711344	47.227572
3503.632216	374218.790430	47.232577
3503.605154	374211.901267	47.237581
3503.670740	374205.277272	47.242586
3503.506183	374204.896482	47.247591
3503.611579	374192.822502	47.252596
3503.639979	374199.025039	47.257601
3503.478405	374207.368945	47.262605
3503.846779	374192.277169	47.267610
3503.545479	374207.358745	47.272615
3503.506520	374195.790903	47.277620
3503.757075	374176.317006	47.282625
3503.607855	374169.726962	47.287629
3503.732759	374158.998093	47.292634
3503.881924	374175.839993	47.297639
3503.713488	374169.354738	47.302644
3503.446028	374168.481459	47.307649
3503.778564	374172.371955	47.312653
3504.024233	374145.165716	47.317658
3503.681930	374142.905186	47.322663
3503.972668	374138.229739	47.327668
3503.849654	374135.451224	47.332673
3503.568986	374131.883620	47.337677
3503.545174	374106.195351	47.342682
3503.619180	374100.689274	47.347687
3503.461893	374092.447032	47.352692
3503.881931	374093.678164	47.357697
3503.411447	374100.213960	47.362701
3503.606403	374086.777584	47.367706
3503.385336	374100.752686	47.372711
3503.358280	374098.900201	47.377716
3503.647648	374107.020213	47.382721
3503.105655	374109.013934	47.387725
3503.185733	374104.397223	47.392730
3503.476158	374117.223071	47.397735
3503.548426	374103.628030	47.402740
3503.685879	374112.357128	47.407745
3503.369004	374113.195995	47.412749
3503.635090	374091.633698	47.417754
3503.698257	374073.537582	47.422759
3503.563781	374090.017350	47.427764
3503.385253	374083.686304	47.432769
3503.229537	374083.787436	47.437773
3503.440986	374083.830524	47.442778
3503.598725	374082.635647	47.447783
3503.695418	374078.703130	47.452788
3503.716721	374079.259597	47.457793
3503.459401	374087.618662	47.462797
3503.649116	374076.447082	47.467802
3503.470193	374063.146116	47.472807
3503.160932	374051.188520	47.477812
3503.370885	374047.823166	47.482817
3503.227283	374040.291012	47.487821
3503.426943	374034.230866	47.492826
3503.244635	374049.395441	47.497831
3503.575766	374060.459656	47.502836
3503.577129	374053.387908	47.507841
3503.079425	374050.083548	47.512845
3503.500382	374047.397099	47.517850
3503.432273	374052.877216	47.522855
3503.370225	374049.173293	47.527860
3503.509472	374052.661911	47.532865
3503.623511	374049.566100	47.537869
3503.470381	374054.576336	47.542874
3503.414356	374054.992401	47.547879
3503.497330	374056.709262	47.552884
3503.451177	374060.456130	47.557889
3503.236444	374061.049911	47.562893
3503.647608	374046.714454	47.567898
3503.482167	374055.873015	47.572903
3503.457630	374065.339991	47.577908
3503.532942	374052.176896	47.582913
3503.710155	374058.686622	47.587917
3503.850009	374030.352330	47.592922
3503.664249	374024.887307	47.597927
3503.762136	374027.975460	47.602932
3503.674147	374026.997493	47.607937
3503.602883	374027.797535	47.612941
3503.668015	374021.860406	47.617946
3503.498390	374019.699762	47.622951
3503.478575	374018.227696	47.627956
3503.567493	373992.648725	47.632961
3503.511178	373997.287533	47.637965
3503.830690	373989.376903	47.642970
3503.195511	373995.073861	47.647975
3503.054517	373991.789420	47.652980
3503.335785	373991.999537	47.657985
3503.022871	374002.605947	47.662989
3503.073321	373986.750341	47.667994
3503.432932	373984.302527	47.672999
3503.565908	373986.571122	47.678004
3503.770471	373994.526497	47.683009
3503.345473	373990.167683	47.688013
3503.620035	373986.664922	47.693018
3503.375543	373997.031575	47.698023
3503.512531	373993.219869	47.703028
3503.498079	374003.804534	47.708033
3503.599482	374012.284972	47.713037
3503.476718	374000.297880	47.718042
3503.378172	373996.396218	47.723047
3503.345296	373998.945410	47.728052
3503.466817	374000.910559	47.733057
3503.344261	374011.944757	47.738061
3503.478801	374011.211428	47.743066
3503.100261	374003.945348	47.748071
3503.581307	373993.465390	47.753076
3503.473106	373979.593582	47.758081
3503.314360	373970.410343	47.763085
3503.398086	373971.618330	47.768090
3503.275836	373978.404351	47.773095
3503.488985	373975.241990	47.778100
3503.640040	373972.191196	47.783105
3503.301531	373979.952608	47.788109
3503.598375	373969.807019	47.793114
3503.746902	373984.461434	47.798119
3503.703438	373974.674899	47.803124
3503.792411	373978.654792	47.808129
3503.296768	373991.147061	47.813133
3503.480421	373974.023934	47.818138
3503.512349	373977.402335	47.823143
3503.544749	373967.451177	47.828148
3503.255465	373950.453680	47.833153
3503.397684	373946.285011	47.838157
3503.667632	373930.852567	47.843162
3503.430447	373947.806512	47.848167
3503.145318	373947.215839	47.853172
3503.319361	373951.589294	47.858177
3503.619021	373950.422854	47.863181
3503.656039	373948.611108	47.868186
3503.401736	373950.508482	47.873191
3503.341029	373942.250942	47.878196
3503.700736	373949.749355	47.883201
3503.595349	373954.319611	47.888205
3503.610730	373956.912053	47.893210
3503.599475	373958.236807	47.898215
3503.605857	373949.866912	47.903220
3503.798513	373921.625949	47.908225
3503.255112	373931.429360	47.913229
3503.597553	373920.309908	47.918234
3503.797766	373926.027442	47.923239
3503.777019	373915.245220	47.928244
3503.487636	373919.208617	47.933249
3503.208362	373922.992350	47.938253
3503.570744	373916.346828	47.943258
3503.550008	373921.946663	47.948263
3503.468612	373939.359305	47.953268
3503.764164	373912.882728	47.958273
3503.658399	373895.321999	47.963277
3503.700504	373892.110357	47.968282
3503.618381	373884.136009	47.973287
3503.772810	373882.280262	47.978292
3503.688274	373886.160403	47.983297
3503.779480	373889.911011	47.988301
3503.900587	373879.258983	47.993306
3503.951602	373860.655934	47.998311
3503.827358	373860.370520	48.003316
3504.367155	373852.323289	48.008321
3503.733670	373843.469450	48.013325
3503.879338	373817.677895	48.018330
3503.806470	373813.339710	48.023335
3503.418293	373814.367922	48.028340
3503.499660	373811.582514	48.033345
3503.458421	373821.128500	48.038349
3503.603246	373812.380559	48.043354
3503.459944	373813.853382	48.048359
3503.485642	373811.534659	48.053364
3503.373599	373794.025756	48.058369
3503.213888	373790.718819	48.063373
3503.373884	373784.842974	48.068378
3503.486362	373796.094455	48.073383
3503.797367	373787.828999	48.078388
3503.785697	373782.845185	48.083393
3503.377418	373781.536273	48.088397
3503.727711	373771.763757	48.093402
3503.562861	373782.550321	48.098407
3503.286294	373778.447839	48.103412
3503.672984	373778.488663	48.108417
3503.546589	373778.941293	48.113421
3503.407658	373781.990587	48.118426
3503.530598	373789.373829	48.123431
3503.466509	373766.057455	48.128436
3503.548042	373757.344945	48.133441
3503.270498	373752.199653	48.138445
3503.526925	373745.901549	48.143450
3503.569050	373757.164162	48.148455
3503.308564	373757.078352	48.153460
3503.343095	373753.359134	48.158465
3503.256758	373751.770385	48.163469
3503.438495	373743.856051	48.168474
3503.477201	373762.190990	48.173479
3503.447716	373750.774155	48.178484
3503.405527	373760.498373	48.183489
3503.435916	373752.964099	48.188493
3503.670162	373765.137547	48.193498
3503.785975	373754.308257	48.198503
3503.529142	373761.929607	48.203508
3503.759358	373765.073175	48.208513
3503.762654	373742.458401	48.213517
3503.508746	373733.035771	48.218522
3503.679799	373729.956360	48.223527
3503.803749	373726.350196	48.228532
3503.582930	373725.444095	48.233537
3503.658359	373736.701449	48.238541
3503.739480	373717.890072	48.243546
3503.558886	373690.725481	48.248551
3503.071131	373686.223927	48.253556
3503.473872	373695.369061	48.258561
3503.480883	373684.785896	48.263565
3503.618059	373683.212687	48.268570
3503.374809	373691.696799	48.273575
3503.428591	373687.821904	48.278580
3503.258605	373696.930386	48.283585
3503.328403	373693.383655	48.288589
3503.593932	373697.259351	48.293594
3503.433243	373696.063925	48.298599
3503.256868	373692.149100	48.303604
3503.400729	373701.258843	48.308609
3503.259837	373688.358754	48.313613
3503.590125	373679.886723	48.318618
3503.406410	373693.398172	48.323623
3503.376531	373690.147017	48.328628
3503.690382	373685.137170	48.333633
3503.465436	373704.989225	48.338637
3503.530572	373698.416097	48.343642
3503.677015	373689.108235	48.348647
3503.511552	373678.119885	48.353652
3503.510690	373666.851131	48.358657
3503.231160	373674.806780	48.363661
3503.542303	373662.547491	48.368666
3503.125523	373669.074865	48.373671
3503.374318	373660.463084	48.378676
3503.641413	373673.318197	48.383681
3503.228965	373676.436175	48.388685
3503.497686	373666.015138	48.393690
3503.636160	373670.674066	48.398695
3503.597406	373673.300521	48.403700
3503.432374	373668.595319	48.408705
3503.348796	373671.025355	48.413709
3503.323875	373668.460245	48.418714
3503.185184	373679.344453	48.423719
3503.336235	373676.929592	48.428724
3503.389083	373673.207472	48.433729
3503.054220	373672.293961	48.438733
3503.372878	373680.180484	48.443738
3503.098449	373681.038088	48.448743
3503.155577	373677.137225	48.453748
3503.559733	373680.355055	48.458753
3503.056956	373688.524060	48.463757
3503.524761	373684.227581	48.468762
3503.421167	373689.865984	48.473767
3503.266801	373686.659947	48.478772
3503.721034	373685.901512	48.483777
3503.542408	373700.531432	48.488781
3503.550803	373686.590217	48.493786
3503.661304	373697.053455	48.498791
3503.883112	373672.572556	48.503796
3503.626540	373653.941724	48.508801
3503.545382	373655.226663	48.513805
3503.465795	373643.410708	48.518810
3503.480093	373655.211949	48.523815
3503.233804	373656.319486	48.528820
3503.715849	373645.584902	48.533825
3503.207565	373655.789836	48.538829
3503.037437	373657.546726	48.543834
3503.234946	373661.051606	48.548839
3503.356440	373658.641416	48.553844
3503.593347	373656.060352	48.558849
3503.186505	373660.144095	48.563853
3503.647103	373655.416303	48.568858
3503.387628	373665.149455	48.573863
3503.511773	373656.201244	48.578868
3503.598026	373649.166883	48.583873
3503.706681	373656.119959	48.588877
3503.698176	373653.908387	48.593882
3503.557177	373639.278505	48.598887
3503.605691	373636.447402	48.603892
3503.804683	373627.614544	48.608897
3503.506214	373642.823069	48.613901
3503.647475	373628.123124	48.618906
3503.304444	373640.845754	48.623911
3503.318610	373640.233201	48.628916
3503.500089	373642.799405	48.633921
3503.257613	373631.823217	48.638925
3503.222944	373639.612975	48.643930
3503.347993	373641.908280	48.648935
3503.714652	373632.565592	48.653940
3503.727913	373638.999550	48.658945
3503.238932	373621.219465	48.663949
3503.414506	373607.506177	48.668954
3503.627919	373595.745643	48.673959
3503.242726	373602.344349	48.678964
3503.586742	373604.605041	48.683969
3503.573299	373601.046023	48.688973
3503.445387	373601.905905	48.693978
3503.580537	373605.293456	48.698983
3503.563119	373603.973626	48.703988
3503.599080	373603.764638	48.708993
3503.085809	373609.544129	48.713997
3503.356528	373611.231330	48.719002
3503.502332	373609.198867	48.724007
3503.270427	373613.738285	48.729012
3503.610799	373609.538257	48.734017
3503.594132	373610.863878	48.739021
3503.664332	373597.879514	48.744026
3503.452690	373590.637853	48.749031
3503.250477	373576.679019	48.754036
3503.646506	373573.920167	48.759041
3503.296900	373577.053656	48.764045
3503.501357	373573.816324	48.769050
3503.261133	373580.239487	48.774055
3503.466128	373573.033712	48.779060
3503.568292	373573.424775	48.784065
3503.303656	373573.950136	48.789069
3503.594773	373575.634114	48.794074
3503.380638	373579.738277	48.799079
3503.714201	373578.286647	48.804084
3503.584026	373575.636417	48.809089
3503.343563	373589.360376	48.814093
3503.696952	373576.789125	48.819098
3503.482117	373586.998563	48.824103
3503.394745	373573.733843	48.829108
3503.734543	373549.590353	48.834113
3503.344482	373545.276845	48.839117
3503.566524	373538.729763	48.844122
3503.468680	373546.376895	48.849127
3503.287773	373543.022413	48.854132
3503.773388	373540.122205	48.859137
3503.326624	373551.716542	48.864141
3503.452970	373548.262612	48.869146
3503.296183	373549.356004	48.874151
3503.210005	373558.247762	48.879156
3503.598959	373546.027014	48.884161
3503.233156	373560.457628	48.889165
3503.641719	373552.583714	48.894170
3503.544474	373551.123873	48.899175
3503.659343	373557.490904	48.904180
3503.824927	373543.779175	48.909185
3503.563700	373532.831364	48.914189
3503.606108	373510.871674	48.919194
3503.797243	373510.790784	48.924199
3503.651930	373511.526227	48.929204
3503.665914	373516.866246	48.934209
3503.566436	373521.944380	48.939213
3503.807208	373512.875949	48.944218
3503.535955	373496.307864	48.949223
3503.422381	373481.749906	48.954228
3503.405827	373474.706329	48.959233
3503.280054	373474.217648	48.964237
3503.372498	373476.721622	48.969242
3503.740457	373479.283795	48.974247
3503.900950	373467.607905	48.979252
3503.410133	373480.989903	48.984257
3503.425825	373487.525254	48.989261
3503.647101	373472.049457	48.994266
3503.698093	373478.706420	48.999271
3503.230552	373477.635811	49.004276
3503.381662	373479.545431	49.009281
3503.148919	373482.202565	49.014285
3503.464635	373480.041483	49.019290
3503.586859	373487.246825	49.024295
3503.253106	373475.191181	49.029300
3503.124813	373466.537218	49.034305
3503.202902	373481.330138	49.039309
3503.359636	373481.025742	49.044314
3503.347309	373489.651458	49.049319
3503.638416	373493.243309	49.054324
3503.593825	373476.334125	49.059329
3503.517346	373450.348515	49.064333
3503.558448	373460.008760	49.069338
3503.267458	373447.488459	49.074343
3503.278115	373452.193055	49.079348
3503.550421	373443.908210	49.084353
3503.291930	373453.412311	49.089357
3503.418613	373443.140863	49.094362
3503.581345	373451.408215	49.099367
3503.229202	373449.556215	49.104372
3503.512799	373453.174695	49.109377
3503.324571	373457.758101	49.114381
3503.390182	373455.509364	49.119386
3503.546544	373456.400624	49.124391
3503.250371	373456.778343	49.129396
3503.626641	373446.747262	49.134401
3503.604397	373457.155231	49.139405
3503.331335	373457.834556	49.144410
3503.437197	373460.819737	49.149415
3503.181732	373468.262857	49.154420
3503.543685	373454.698123	49.159425
3503.318552	373460.330332	49.164429
3503.231783	373467.594154	49.169434
3503.391513	373461.489361	49.174439
3503.598369	373464.077003	49.179444
3503.490106	373446.516478	49.184449
3503.107079	373444.160594	49.189453
3503.640264	373438.556402	49.194458
3503.718170	373435.339065	49.199463
3503.323177	373431.560529	49.204468
3503.540188	373419.392363	49.209473
3503.401581	373426.995085	49.214477
3503.454731	373422.815006	49.219482
3503.530396	373427.407575	49.224487
3503.518306	373426.214089	49.229492
3503.546603	373420.587956	49.234497
3503.643188	373430.061368	49.239501
3503.802425	373422.811925	49.244506
3503.592044	373425.643595	49.249511
3503.198274	373402.353695	49.254516
3503.281580	373389.061934	49.259521
3503.095490	373398.605479	49.264525
3503.530075	373415.631513	49.269530
3503.119968	373413.941304	49.274535
3503.469028	373419.279242	49.279540
3503.603880	373404.198657	49.284545
3503.544558	373404.564372	49.289549
3503.607207	373392.929367	49.294554
3503.706564	373407.032117	49.299559
3503.763652	373404.454026	49.304564
3504.020746	373397.774190	49.309569
3503.537627	373398.232339	49.314573
3503.669574	373387.553033	49.319578
3503.447390	373368.535062	49.324583
3503.473405	373363.214542	49.329588
3503.683960	373365.241962	49.334593
3503.445736	373362.328978	49.339597
3503.380899	373357.175449	49.344602
3503.758644	373357.522949	49.349607
3503.458726	373369.882710	49.354612
3503.568726	373365.337501	49.359617
3503.559817	373370.045200	49.364621
3502.963260	373363.271361	49.369626
3503.637855	373368.557844	49.374631
3503.260523	373372.077307	49.379636
3503.620104	373365.890030	49.384641
3503.214143	373382.514750	49.389645
3503.380298	373376.765065	49.394650
3503.805620	373379.445367	49.399655
3503.560301	373364.577497	49.404660
3503.790748	373349.710725	49.409665
3503.650004	373337.217516	49.414669
3503.655168	373329.432769	49.419674
3503.454201	373343.226881	49.424679
3503.372708	373348.175001	49.429684
3503.541797	373341.763451	49.434689
3503.218582	373348.428714	49.439693
3503.448828	373345.848684	49.444698
3503.411764	373344.023185	49.449703
3503.253002	373350.001054	49.454708
3503.412164	373344.125278	49.459713
3503.157347	373351.848138	49.464717
3503.335240	373340.296653	49.469722
3503.207947	373352.832636	49.474727
3503.616899	373337.428875	49.479732
3503.877100	373341.178255	49.484737
3503.208076	373328.158035	49.489741
3503.446049	373310.084828	49.494746
3503.758801	373304.846164	49.499751
3503.482444	373314.302244	49.504756
3503.682941	373316.433010	49.509761
3503.562285	373308.820780	49.514765
3503.488421	373307.255480	49.519770
3503.387357	373315.997013	49.524775
3503.340170	373323.203726	49.529780
3503.418829	373310.014428	49.534785
3503.416334	373308.158024	49.539789
3503.742706	373318.231095	49.544794
3503.830891	373313.943713	49.549799
3503.519110	373303.283655	49.554804
3503.462268	373291.692949	49.559809
3503.484779	373281.590560	49.564813
3503.895640	373273.385531	49.569818
3503.931607	373278.213338	49.574823
3503.649416	373279.479192	49.579828
3504.060244	373274.479403	49.584833
3503.443171	373261.578142	49.589837
3503.735199	373239.807793	49.594842
3503.536383	373244.036760	49.599847
3503.545576	373236.454866	49.604852
3503.641095	373236.821543	49.609857
3503.575757	373253.239838	49.614861
3503.775423	373233.926172	49.619866
3503.774708	373241.354499	49.624871
3503.626809	373237.180745	49.629876
3503.501205	373211.838712	49.634881
3503.380757	373208.957975	49.639885
3503.520737	373199.981724	49.644890
3503.642221	373199.479391	49.649895
3503.544136	373205.600319	49.654900
3503.777636	373198.720673	49.659905
3503.361046	373198.023578	49.664909
3503.978654	373192.533200	49.669914
3503.561912	373195.219439	49.674919
3503.452753	373180.279101	49.679924
3503.397315	373164.668865	49.684929
3503.289113	373166.568616	49.689933
3503.406065	373163.472278	49.694938
3503.246148	373170.569647	49.699943
3503.052744	373177.952130	49.704948
3503.457238	373161.734979	49.709953
3503.093355	373169.475114	49.714957
3503.513105	373176.811545	49.719962
3503.124039	373173.515378	49.724967
3503.038982	373184.492990	49.729972
3503.501178	373203.829644	49.734977
3503.162981	373218.688466	49.739981
3503.456675	373208.899327	49.744986
3503.345349	373218.685478	49.749991
3503.175789	373217.058988	49.754996
3503.698482	373214.737980	49.760001
3503.432437	373199.110174	49.765005
3503.694026	373189.402421	49.770010
3503.695128	373178.311292	49.775015
3503.140323	373191.525429	49.780020
3503.600413	373185.042414	49.785025
3503.586931	373176.497433	49.790029
3503.668644	373183.276779	49.795034
3503.457635	373188.321708	49.800039
3503.585058	373185.757923	49.805044
3504.089751	373171.610887	49.810049
3503.536032	373168.671448	49.815053
3503.578620	373165.357920	49.820058
3503.671852	373154.684674	49.825063
3503.151118	373155.377718	49.830068
3503.344999	373149.242042	49.835073
3503.342675	373161.631135	49.840077
3503.237405	373160.350618	49.845082
3503.360798	373160.738328	49.850087
3503.658382	373155.145904	49.855092
3503.691006	373153.054996	49.860097
3503.275565	373170.800591	49.865101
3503.616429	373164.590804	49.870106
3503.504745	373163.565685	49.875111
3503.250182	373164.598228	49.880116
3503.620926	373166.091566	49.885121
3503.723315	373164.879974	49.890125
3503.607718	373142.665245	49.895130
3503.754049	373138.572161	49.900135
3503.630556	373120.123560	49.905140
3503.815373	373118.262975	49.910145
3503.245536	373121.456751	49.915149
3503.351790	373113.757738	49.920154
3503.763032	373115.066606	49.925159
3503.453726	373117.684989	49.930164
3503.434225	373122.674214	49.935169
3503.295304	373130.124408	49.940173
3503.401796	373121.433258	49.945178
3503.487444	373130.450576	49.950183
3503.404042	373125.045568	49.955188
3503.329909	373090.461160	49.960193
3503.233744	373098.718633	49.965197
3503.461982	373097.919599	49.970202
3503.507263	373092.417929	49.975207
3503.038190	373085.471261	49.980212
3503.375850	373083.484758	49.985217
3503.457077	373087.847539	49.990221
3503.386422	373083.941383	49.995226
3503.391353	373085.339922	50.000231
3503.364099	373095.138250	50.005236
3503.799423	373089.600359	50.010241
3503.297271	373102.500938	50.015245
3503.372121	373085.623591	50.020250
3503.418090	373094.214735	50.025255
3503.254819	373090.628482	50.030260
3503.669605	373095.396425	50.035265
3503.666543	373105.750572	50.040269
3503.773210	373095.533080	50.045274
3503.876239	373102.181877	50.050279
3503.479403	373085.429973	50.055284
3503.672578	373056.399746	50.060289
3503.579469	373072.008470	50.065293
3503.614843	373054.399634	50.070298
3503.645331	373056.175711	50.075303
3503.378701	373062.246989	50.080308
3503.707119	373057.234764	50.085313
3503.307650	373068.440180	50.090317
3503.265029	373056.745407	50.095322
3503.269075	373061.374777	50.100327
3502.989591	373052.235859	50.105332
3503.396059	373064.560358	50.110337
3503.206758	373067.617666	50.115341
3503.336004	373063.552714	50.120346
3503.193570	373061.820175	50.125351
3503.185769	373064.848792	50.130356
3503.290426	373065.875427	50.135361
3503.101085	373070.255544	50.140365
3503.619034	373067.553701	50.145370
3503.382972	373068.303498	50.150375
3503.462115	373070.148199	50.155380
3503.655734	373066.302017	50.160385
3503.313944	373071.469389	50.165389
3503.211229	373065.685849	50.170394
3503.298271	373069.437189	50.175399
3503.143602	373061.016258	50.180404
3503.033528	373055.030373	50.185409
3503.088936	373073.286661	50.190413
3503.474911	373072.513568	50.195418
3503.574966	373074.838294	50.200423
3503.298964	373074.297042	50.205428
3503.535890	373071.054538	50.210433
3503.673309	373076.680363	50.215437
3503.505415	373087.035134	50.220442
3503.477201	373080.629295	50.225447
3503.803028	373077.652562	50.230452
3503.660149	373069.026261	50.235457
3503.335216	373054.959458	50.240461
3503.422999	373044.973886	50.245466
3503.218414	373047.855543	50.250471
3503.067073	373045.742833	50.255476
3503.421418	373043.702814	50.260481
3503.265382	373053.750457	50.265485
3503.286745	373052.322725	50.270490
3503.654440	373042.038516	50.275495
3503.527552	373044.500875	50.280500
3503.388644	373037.425689	50.285505
3503.203347	373048.291991	50.290509
3503.544726	373048.238226	50.295514
3503.677923	373046.385798	50.300519
3503.449623	373046.727352	50.305524
3503.549617	373044.727542	50.310529
3503.670295	373045.446383	50.315533
3503.685293	373047.988065	50.320538
3503.525776	373055.110828	50.325543
3503.433862	373056.295731	50.330548
3503.484520	373042.016919	50.335553
3503.111734	373036.759401	50.340557
3503.204426	373036.363372	50.345562
3503.409907	373043.555629	50.350567
3503.458044	373039.401743	50.355572
3503.672813	373023.061899	50.360577
3503.455146	373015.490389	50.365581
3503.527023	373009.424856	50.370586
3503.792483	373013.402381	50.375591
3503.922498	373008.803093	50.380596
3503.880222	373004.154725	50.385601
3503.673499	373014.057759	50.390605
3503.519512	372999.556897	50.395610
3503.675353	372979.792148	50.400615
3503.267345	372984.384912	50.405620
3503.471645	372970.030909	50.410625
3503.467368	372977.180022	50.415629
3503.202116	372981.165132	50.420634
3503.229061	372988.309307	50.425639
3503.199991	372983.200955	50.430644
3503.405029	372970.881920	50.435649
3503.269521	372984.513171	50.440653
3503.447690	372983.264156	50.445658
3503.617957	372977.590082	50.450663
3503.659551	372991.549473	50.455668
3503.617913	372985.934338	50.460673
3503.837751	372983.355931	50.465677
3503.663735	372986.588899	50.470682
3503.480445	372980.538261	50.475687
3503.654652	372967.003049	50.480692
3503.761626	372952.537233	50.485697
3503.502978	372948.406396	50.490701
3503.483410	372953.497406	50.495706
3503.306127	372945.283535	50.500711
3503.163702	372951.106247	50.505716
3503.471515	372953.347259	50.510721
3503.612689	372951.391812	50.515725
3503.500103	372947.950165	50.520730
3503.604718	372944.626814	50.525735
3503.215256	372913.551753	50.530740
3503.449776	372869.175384	50.535745
3503.257323	372842.953342	50.540749
3503.183945	372783.260615	50.545754
3503.118066	372725.449082	50.550759
3502.770127	372662.365359	50.555764
3502.666763	372590.084914	50.560769
3502.340946	372510.513124	50.565773
3501.904653	372421.113797	50.570778
3501.640859	372318.204363	50.575783
3501.396769	372229.588289	50.580788
3501.404101	372109.413268	50.585793
3500.557444	372014.913813	50.590797
3500.530984	371887.289830	50.595802
3500.328509	371765.264492	50.600807
3499.521560	371645.929175	50.605812
3499.641478	371515.355401	50.610817
3498.942110	371369.875982	50.615821
3498.565205	371230.247077	50.620826
3497.971106	371082.307826	50.625831
3497.538093	370927.422971	50.630836
3497.150551	370770.495172	50.635841
3496.643778	370634.039386	50.640845
3496.449904	370458.635843	50.645850
3495.710020	370291.331552	50.650855
3495.134831	370144.403667	50.655860
3494.802719	369965.305679	50.660865
3494.221472	369792.250282	50.665869
3493.657435	369620.870546	50.670874
3493.024892	369445.455893	50.675879
3492.281547	369273.339905	50.680884
3491.918449	369087.603130	50.685889
3491.227409	368912.551739	50.690893
3490.740738	368730.547358	50.695898
3490.222926	368547.173314	50.700903
3489.788024	368350.428705	50.705908
3489.251383	368159.016553	50.710913
3488.572268	367977.904469	50.715917
3488.145847	367772.734779	50.720922
3487.457092	367584.168194	50.725927
3486.455405	367395.548506	50.730932
3486.415512	367194.970884	50.735937
3485.602947	366986.551129	50.740941
3484.836307	366798.731330	50.745946
3484.323359	366585.962597	50.750951
3483.359452	366393.109249	50.755956
3483.193583	366184.150981	50.760961
3482.410849	365989.842469	50.765965
3481.150864	365794.768955	50.770970
3480.996083	365589.826126	50.775975
3480.297563	365391.532625	50.780980
3479.844566	365180.655978	50.785985
3479.107184	364987.659019	50.790989
3478.179119	364777.771560	50.795994
3477.822194	364575.196887	50.800999
3476.967617	364383.869720	50.806004
3476.386211	364174.001008	50.811009
3475.454330	363971.819882	50.816013
3475.124104	363769.161089	50.821018
3474.738555	363553.228367	50.826023
3473.648146	363364.275085	50.831028
3473.085973	363154.296904	50.836033
3472.374595	362952.865223	50.841037
3472.029108	362734.886801	50.846042
3471.370994	362535.989341	50.851047
3470.504533	362322.391490	50.856052
3470.381002	362114.273069	50.861057
3469.109878	361915.469886	50.866061
3468.676493	361697.653197	50.871066
3467.795163	361485.809599	50.876071
3466.979313	361279.425432	50.881076
3466.858993	361062.039778	50.886081
3466.083486	360850.023932	50.891085
3465.189131	360643.445847	50.896090
3464.808743	360450.017381	50.901095
3464.156635	360235.154819	50.906100
3463.319243	360011.643521	50.911105
3462.625483	359813.249179	50.916109
3461.881992	359586.184058	50.921114
3461.588228	359378.793082	50.926119
3460.713923	359172.154610	50.931124
3460.038341	358962.633832	50.936129
3459.452952	358758.314446	50.941133
3458.760450	358532.203304	50.946138
3458.011389	358320.553862	50.951143
3457.348111	358099.983513	50.956148
3456.885625	357888.515922	50.961153
3455.927404	357681.731739	50.966157
3455.358020	357466.436719	50.971162
3454.630247	357256.611546	50.976167
3453.819489	357049.597831	50.981172
3453.204321	356835.605138	50.986177
3452.906297	356625.887496	50.991181
3451.857557	356406.897426	50.996186
3451.390070	356201.785409	51.001191
3450.808219	355991.550138	51.006196
3450.173931	355769.361659	51.011201
3449.219341	355567.250613	51.016205
3448.695493	355348.580132	51.021210
3448.350919	355147.007175	51.026215
3447.062702	354930.975150	51.031220
3446.709728	354713.140179	51.036225
3445.662469	354518.470636	51.041229
3445.163015	354290.604772	51.046234
3444.586082	354091.253005	51.051239
3443.734493	353879.397503	51.056244
3443.435262	353655.798077	51.061249
3442.445752	353464.449275	51.066253
3441.724114	353255.548247	51.071258
3441.221860	353045.822763	51.076263
3439.993117	352836.872995	51.081268
3439.875945	352618.584756	51.086273
3439.087887	352423.357396	51.091277
3438.376581	352200.096858	51.096282
3437.565065	352000.087064	51.101287
3436.636631	351788.133464	51.106292
3436.169562	351588.169460	51.111297
3435.616572	351385.393311	51.116301
3434.762202	351183.529359	51.121306
3434.360605	350977.037423	51.126311
3433.371230	350774.887876	51.131316
3432.742063	350562.118591	51.136321
3432.148402	350373.088417	51.141325
3431.832229	350163.245816	51.146330
3430.991402	349959.186374	51.151335
3430.028101	349746.568531	51.156340
3429.798108	349544.828808	51.161345
3428.816150	349339.694971	51.166349
3427.863168	349132.901450	51.171354
3427.271574	348929.435052	51.176359
3426.528017	348741.924583	51.181364
3426.126100	348529.035114	51.186369
3425.344103	348326.665578	51.191373
3424.749373	348129.865093	51.196378
3424.084184	347928.264650	51.201383
3423.228759	347721.832234	51.206388
3422.873647	347520.613982	51.211393
3422.086891	347322.339357	51.216397
3421.336515	347124.414616	51.221402
3420.941499	346921.902478	51.226407
3420.209920	346713.156087	51.231412
3419.310183	346519.707033	51.236417
3418.742188	346300.726807	51.241421
3418.025052	346105.414893	51.246426
3417.346151	345911.419814	51.251431
3416.385987	345715.025080	51.256436
3415.901528	345503.740836	51.261441
3415.134582	345301.994480	51.266445
3414.513340	345110.787438	51.271450
3414.183462	344906.679821	51.276455
3413.212201	344709.494397	51.281460
3412.630836	344505.781495	51.286465
3411.899603	344304.789655	51.291469
3411.392461	344108.368794	51.296474
3410.974954	343904.704268	51.301479
3409.569823	343723.390874	51.306484
3409.511931	343501.086871	51.311489
3408.812300	343310.853638	51.316493
3407.918471	343106.701719	51.321498
3407.218383	342908.983808	51.326503
3406.490660	342706.509688	51.331508
3405.971657	342501.634640	51.336513
3405.274105	342310.176115	51.341517
3404.508116	342109.615127	51.346522
3404.100648	341907.800425	51.351527
3402.947805	341716.157483	51.356532
3402.743989	341512.680183	51.361537
3402.034906	341317.300353	51.366541
3401.204582	341112.164420	51.371546
3400.365648	340906.850985	51.376551
3399.779152	340719.213632	51.381556
3399.427916	340508.476213	51.386561
3398.342973	340326.822075	51.391565
3397.780287	340117.618630	51.396570
3397.209549	339921.881626	51.401575
3396.368217	339734.739816	51.406580
3395.917484	339527.324041	51.411585
3395.208785	339328.908737	51.416589
3394.099868	339140.789264	51.421594
3393.802566	338942.256790	51.426599
3393.356990	338749.729256	51.431604
3392.741186	338547.325732	51.436609
3391.941009	338361.522546	51.441613
3391.268089	338145.482408	51.446618
3390.678472	337945.007513	51.451623
3389.812843	337756.947350	51.456628
3389.288676	337557.504616	51.461633
3388.741339	337357.886744	51.466637
3388.020361	337159.874020	51.471642
3387.498204	336959.920024	51.476647
3386.727643	336767.107085	51.481652
3386.228985	336559.282085	51.486657
3385.050100	336364.521471	51.491661
3384.343218	336172.282240	51.496666
3383.985188	335965.629621	51.501671
3383.047850	335769.734433	51.506676
3382.309534	335563.395284	51.511681
3381.855090	335377.452659	51.516685
3381.010837	335180.420931	51.521690
3380.602735	334986.018128	51.526695
3379.606389	334790.103983	51.531700
3379.192093	334582.412295	51.536705
3378.021513	334403.530130	51.541709
3377.881659	334199.637962	51.546714
3377.320770	334011.824605	51.551719
3376.492618	333823.212900	51.556724
3375.776374	333624.450808	51.561729
3375.078325	333424.590588	51.566733
3374.383716	333220.783282	51.571738
3373.940289	333027.653462	51.576743
3372.929173	332838.457049	51.581748
3372.704116	332639.563581	51.586753
3371.812395	332452.816693	51.591757
3371.018106	332251.389967	51.596762
3370.747858	332050.414427	51.601767
3369.630823	331864.872716	51.606772
3369.172037	331668.584805	51.611777
3368.638856	331469.100354	51.616781
3367.902426	331277.692406	51.621786
3367.090047	331077.258146	51.626791
3366.498230	330887.251987	51.631796
3366.057350	330689.685668	51.636801
3364.857693	330494.581027	51.641805
3364.539520	330300.100236	51.646810
3363.996873	330094.834367	51.651815
3363.090860	329914.728018	51.656820
3362.408403	329712.156403	51.661825
3361.764012	329521.213066	51.666829
3361.304287	329327.032175	51.671834
3360.610511	329127.770475	51.676839
3359.886556	328927.621946	51.681844
3359.221975	328736.425224	51.686849
3358.474487	328542.338749	51.691853
3357.935134	328344.730905	51.696858
3357.247620	328152.390669	51.701863
3356.337130	327964.031469	51.706868
3355.708496	327765.647009	51.711873
3355.169612	327564.829163	51.716877
3354.316401	327379.158228	51.721882
3353.638753	327187.654217	51.726887
3352.907334	326989.436798	51.731892
3352.320018	326798.401294	51.736897
3351.347117	326610.176003	51.741901
3350.770052	326424.408225	51.746906
3350.417275	326222.590038	51.751911
3349.450699	326036.144609	51.756916
3349.093883	325854.312484	51.761921
3348.010700	325663.149001	51.766925
3347.418419	325472.747625	51.771930
3347.085092	325276.754448	51.776935
3346.606627	325097.842368	51.781940
3345.921908	324907.046920	51.786945
3345.168784	324714.708741	51.791949
3344.136229	324523.738268	51.796954
3343.927232	324332.127890	51.801959
3343.019941	324144.752173	51.806964
3342.367952	323940.302269	51.811969
3341.636732	323753.865347	51.816973
3340.819903	323562.985861	51.821978
3340.268658	323370.307120	51.826983
3339.641897	323192.534688	51.831988
3339.296953	323004.736502	51.836993
3338.490785	322809.066917	51.841997
3337.483468	322620.888880	51.847002
3337.208155	322422.079092	51.852007
3336.362010	322233.467336	51.857012
3335.685035	322043.631723	51.862017
3334.695134	321853.666956	51.867021
3333.999486	321667.576332	51.872026
3333.661533	321474.885085	51.877031
3332.821086	321295.945854	51.882036
3332.727516	321101.432818	51.887041
3331.962843	320924.212256	51.892045
3331.103728	320732.009210	51.897050
3330.129955	320522.076889	51.902055
3329.317479	320346.772394	51.907060
3328.837766	320161.688416	51.912065
3328.173994	319969.554698	51.917069
3327.659233	319784.679193	51.922074
3327.199830	319592.766982	51.927079
3325.840920	319405.910857	51.932084
3325.416909	319218.957415	51.937089
3324.981352	319033.125768	51.942093
3324.119275	318846.750110	51.947098
3323.570048	318654.926551	51.952103
3322.988294	318475.864480	51.957108
3322.231741	318286.440977	51.962113
3321.493871	318105.875140	51.967117
3320.654113	317922.880657	51.972122
3320.427031	317737.981067	51.977127
3319.608935	317544.848263	51.982132
3319.041221	317363.439305	51.987137
3318.485043	317173.370800	51.992141
3317.724232	316984.149102	51.997146
3316.999172	316793.037122	52.002151
3316.384785	316604.275328	52.007156
3315.890228	316420.994247	52.012161
3315.240377	316226.151662	52.017165
3314.552005	316026.705951	52.022170
3313.805252	315842.674333	52.027175
3312.903117	315657.928519	52.032180
3312.426063	315468.302565	52.037185
3311.727422	315273.109361	52.042189
3310.698934	315082.729612	52.047194
3310.068008	314905.858659	52.052199
3309.331861	314717.138046	52.057204
3309.019196	314529.088551	52.062209
3308.386268	314354.636008	52.067213
3307.736562	314167.199367	52.072218
3307.306220	313979.880476	52.077223
3306.074977	313791.363813	52.082228
3305.711750	313603.116943	52.087233
3305.326615	313419.100201	52.092237
3304.554209	313228.065438	52.097242
3304.202583	313034.213678	52.102247
3303.220536	312845.986962	52.107252
3302.729504	312651.163470	52.112257
3301.785889	312460.765568	52.117261
3301.025904	312272.986556	52.122266
3300.429568	312075.275788	52.127271
3299.468466	311905.734823	52.132276
3299.199091	311711.332963	52.137281
3298.537158	311526.134529	52.142285
3297.845162	311335.491182	52.147290
3296.942964	311140.959250	52.152295
3296.483952	310954.963853	52.157300
3295.468094	310762.028044	52.162305
3295.220330	310583.383316	52.167309
3294.150488	310404.257193	52.172314
3293.944326	310206.659699	52.177319
3293.000702	310018.905996	52.182324
3292.503214	309838.975464	52.187329
3291.745390	309651.166320	52.192333
3290.958742	309466.111627	52.197338
3290.436610	309268.129637	52.202343
3289.617482	309093.265409	52.207348
3288.948121	308902.410783	52.212353
3287.982419	308716.059084	52.217357
3287.289029	308534.553292	52.222362
3286.929170	308353.274588	52.227367
3286.005663	308171.015244	52.232372
3285.378253	307983.997764	52.237377
3285.168973	307809.417215	52.242381
3284.375808	307631.159943	52.247386
3283.442631	307435.251756	52.252391
3282.717250	307256.932304	52.257396
3282.071844	307069.508869	52.262401
3281.620028	306893.488437	52.267405
3280.820557	306717.268103	52.272410
3280.132554	306523.891734	52.277415
3279.443811	306350.530969	52.282420
3278.700017	306166.152168	52.287425
3277.982320	305998.270578	52.292429
3277.467027	305817.725890	52.297434
3277.061367	305624.685523	52.302439
3276.110343	305465.982284	52.307444
3275.471508	305274.327970	52.312449
3275.126487	305088.891448	52.317453
3274.486207	304913.916821	52.322458
3273.764220	304722.987924	52.327463
3272.960577	304541.213866	52.332468
3272.495457	304358.341928	52.337473
3271.927552	304164.382934	52.342477
3271.251530	303979.379273	52.347482
3270.757760	303797.122317	52.352487
3269.780011	303611.631122	52.357492
3269.365686	303421.695895	52.362497
3268.613675	303236.652362	52.367501
3267.434347	303056.336459	52.372506
3267.334968	302867.649454	52.377511
3266.313035	302700.677866	52.382516
3265.346679	302503.647351	52.387521
3265.067886	302326.193104	52.392525
3264.385777	302141.035278	52.397530
3263.939839	301945.526076	52.402535
3263.018568	301767.714413	52.407540
3262.507773	301591.798513	52.412545
3261.570064	301406.807562	52.417549
3260.673717	301223.363291	52.422554
3260.386876	301032.946489	52.427559
3259.702509	300858.177736	52.432564
3259.090989	300676.903345	52.437569
3258.371378	300495.747714	52.442573
3257.569206	300321.353540	52.447578
3257.018951	300129.729477	52.452583
3256.060063	299956.123697	52.457588
3255.464446	299777.850831	52.462593
3255.055843	299591.297035	52.467597
3254.301128	299409.865627	52.472602
3253.331668	299230.912786	52.477607
3253.124508	299055.761027	52.482612
3252.301896	298875.256587	52.487617
3251.559857	298699.195877	52.492621
3250.588546	298513.010048	52.497626
3250.248121	298325.781952	52.502631
3249.214280	298158.196342	52.507636
3248.897935	297989.249202	52.512641
3248.225656	297805.714802	52.517645
3247.320055	297627.641557	52.522650
3246.844716	297445.323512	52.527655
3246.111482	297272.341489	52.532660
3245.148354	297095.855774	52.537665
3244.793604	296915.886551	52.542669
3244.107275	296745.494244	52.547674
3243.495361	296566.838717	52.552679
3242.325238	296403.169513	52.557684
3242.028347	296220.516446	52.562689
3241.423855	296046.366921	52.567693
3240.526062	295882.348594	52.572698
3240.369879	295690.428231	52.577703
3239.427192	295524.583080	52.582708
3238.984583	295330.492045	52.587713
3237.911083	295164.616357	52.592717
3237.457084	294983.387701	52.597722
3237.479906	294806.616613	52.602727
3236.841986	294635.323483	52.607732
3236.056265	294444.418360	52.612737
3235.054939	294259.226370	52.617741
3234.200743	294087.126592	52.622746
3233.748226	293905.565700	52.627751
3232.955193	293726.401518	52.632756
3232.116244	293550.733480	52.637761
3231.239553	293376.879457	52.642765
3230.598985	293204.617856	52.647770
3230.657125	293020.912598	52.652775
3229.261277	292845.765058	52.657780
3228.986839	292676.985109	52.662785
3228.587570	292507.919177	52.667789
3227.722611	292320.106334	52.672794
3227.178975	292129.390150	52.677799
3226.627748	291949.549644	52.682804
3225.679511	291768.371097	52.687809
3224.884487	291594.197224	52.692813
3223.911903	291417.835640	52.697818
3223.674840	291241.535845	52.702823
3222.627169	291071.349053	52.707828
3222.159161	290884.389155	52.712833
3221.453137	290711.957862	52.717837
3220.580866	290546.632765	52.722842
3220.542627	290369.893441	52.727847
3219.352613	290206.503009	52.732852
3219.062702	290007.722779	52.737857
3218.290728	289849.665152	52.742861
3217.576028	289665.875963	52.747866
3217.043198	289483.407671	52.752871
3216.078890	289315.371346	52.757876
3215.348087	289133.978331	52.762881
3214.891041	288956.260193	52.767885
3214.231948	288783.896686	52.772890
3213.648888	288610.858887	52.777895
3212.838660	288446.006639	52.782900
3212.231439	288261.766615	52.787905
3211.716935	288091.213529	52.792909
3210.711582	287928.174628	52.797914
3210.317180	287743.034724	52.802919
3209.353860	287579.250428	52.807924
3208.757612	287392.257634	52.812929
3208.049116	287226.217139	52.817933
3207.174787	287065.423729	52.822938
3206.787082	286884.000609	52.827943
3205.722163	286716.895667	52.832948
3205.347741	286539.264996	52.837953
3204.986170	286384.324193	52.842957
3204.434254	286201.296753	52.847962
3204.003139	286025.890519	52.852967
3202.943997	285851.958837	52.857972
3201.950243	285679.009984	52.862977
3201.578343	285510.164901	52.867981
3201.016105	285334.626288	52.872986
3200.696573	285163.200497	52.877991
3200.048590	284981.053596	52.882996
3199.104947	284799.539159	52.888001
3198.124074	284627.886694	52.893005
3197.470700	284461.479716	52.898010
3197.062318	284278.097607	52.903015
3196.273688	284109.012274	52.908020
3195.482011	283924.417256	52.913025
3195.225087	283751.274638	52.918029
3194.396881	283574.223838	52.923034
3193.774939	283395.459440	52.928039
3193.069291	283225.876769	52.933044
3192.378244	283054.941917	52.938049
3191.825087	282877.669077	52.943053
3190.854697	282699.035971	52.948058
3190.512964	282514.114564	52.953063
3189.838764	282351.021035	52.958068
3188.953303	282187.171369	52.963073
3188.322002	282011.311369	52.968077
3187.554498	281848.054184	52.973082
3187.003223	281662.936445	52.978087
3185.834064	281505.574950	52.983092
3185.492662	281325.211942	52.988097
3184.953947	281153.794002	52.993101
3184.240523	280985.383449	52.998106
3183.603663	280807.919499	53.003111
3182.821903	280647.440318	53.008116
3182.119322	280472.686325	53.013121
3181.637984	280302.430646	53.018125
3180.436000	280137.637298	53.023130
3180.488890	279955.632532	53.028135
3179.779036	279793.180742	53.033140
3178.855876	279615.481673	53.038145
3178.267822	279451.558854	53.043149
3177.241651	279277.721738	53.048154
3176.730102	279118.676681	53.053159
3176.237514	278946.003033	53.058164
3175.634703	278772.378999	53.063169
3175.013458	278613.478565	53.068173
3174.273558	278445.020781	53.073178
3173.563274	278266.294538	53.078183
3172.717747	278100.629473	53.083188
3172.290973	277928.913065	53.088193
3171.876541	277759.257622	53.093197
3171.077667	277588.975343	53.098202
3170.158368	277414.968249	53.103207
3169.589002	277252.366542	53.108212
3168.773599	277078.215637	53.113217
3168.291161	276901.541601	53.118221
3167.443915	276746.089501	53.123226
3167.262866	276571.328820	53.128231
3166.250348	276409.663097	53.133236
3165.963245	276237.083990	53.138241
3165.030670	276058.723808	53.143245
3164.216492	275887.170414	53.148250
3163.692464	275713.788318	53.153255
3162.625829	275546.731829	53.158260
3162.246182	275368.462418	53.163265
3161.413477	275213.058904	53.168269
3160.624084	275041.730790	53.173274
3160.446069	274873.718705	53.178279
3159.349067	274713.721765	53.183284
3158.889853	274547.842587	53.188289
3158.715690	274378.403672	53.193293
3157.612466	274211.505795	53.198298
3156.999318	274045.523647	53.203303
3156.256829	273881.166481	53.208308
3155.642706	273707.238368	53.213313
3154.876221	273544.031095	53.218317
3153.976189	273371.217916	53.223322
3153.542444	273210.810475	53.228327
3152.730640	273043.331721	53.233332
3152.178161	272879.810484	53.238337
3151.605436	272706.716356	53.243341
3150.704269	272550.126785	53.248346
3150.075155	272385.751798	53.253351
3149.332125	272209.704874	53.258356
3148.776985	272044.579638	53.263361
3148.291009	271873.407479	53.268365
3147.609627	271720.323326	53.273370
3147.571437	271546.788206	53.278375
3146.408010	271379.441692	53.283380
3145.693730	271207.669047	53.288385
3145.123525	271035.211457	53.293389
3144.292268	270872.142084	53.298394
3143.870005	270707.607263	53.303399
3142.664939	270539.885456	53.308404
3142.146013	270370.883566	53.313409
3141.713933	270201.740627	53.318413
3140.671327	270042.601503	53.323418
3140.022700	269873.289151	53.328423
3139.528602	269717.628862	53.333428
3139.034309	269545.286902	53.338433
3138.409909	269377.015029	53.343437
3137.601940	269220.869678	53.348442
3136.748657	269049.119479	53.353447
3135.986536	268895.844864	53.358452
3135.495032	268725.591067	53.363457
3134.677971	268566.900484	53.368461
3133.975760	268414.686172	53.373466
3133.470351	268240.359788	53.378471
3132.867688	268085.735793	53.383476
3131.964585	267921.608794	53.388481
3131.633877	267760.549327	53.393485
3131.007097	267594.061091	53.398490
3130.651856	267438.735949	53.403495
3129.660346	267272.127251	53.408500
3128.957066	267102.085728	53.413505
3128.283486	266932.956417	53.418509
3127.516306	266781.771569	53.423514
3127.198904	266609.377017	53.428519
3126.370670	266453.872346	53.433524
3125.439197	266281.243999	53.438529
3124.791257	266109.767853	53.443533
3123.968443	265957.395074	53.448538
3123.295688	265796.492248	53.453543
3122.890549	265641.353863	53.458548
3122.185684	265479.437513	53.463553
3121.470556	265312.327358	53.468557
3120.642521	265159.726476	53.473562
3120.262592	264994.702726	53.478567
3119.907972	264830.948442	53.483572
3118.780781	264668.844563	53.488577
3118.272406	264496.608421	53.493581
3117.495002	264339.008108	53.498586
3117.007985	264176.548454	53.503591
3115.897033	264019.434015	53.508596
3115.579121	263859.188925	53.513601
3115.085345	263690.007005	53.518605
3114.175338	263530.263247	53.523610
3113.430985	263374.186201	53.528615
3112.715527	263219.607263	53.533620
3112.049737	263059.570396	53.538625
3111.651853	262891.621620	53.543629
3110.877675	262736.746580	53.548634
3110.332413	262577.072890	53.553639
3109.356648	262428.367662	53.558644
3108.833991	262252.060025	53.563649
3108.329483	262091.641559	53.568653
3107.663383	261942.174455	53.573658
3106.925087	261771.325866	53.578663
3106.004816	261617.798821	53.583668
3105.567226	261458.490681	53.588673
3104.993778	261301.954648	53.593677
3104.446551	261134.616209	53.598682
3103.711926	260973.954609	53.603687
3102.788543	260814.494487	53.608692
3102.143080	260656.442134	53.613697
3101.501932	260496.886591	53.618701
3100.761418	260342.032923	53.623706
3100.339688	260174.445982	53.628711
3099.522401	260012.702905	53.633716
3099.068950	259851.691845	53.638721
3098.312250	259683.037642	53.643725
3097.367888	259530.279580	53.648730
3096.762809	259372.068780	53.653735
3095.972179	259233.472028	53.658740
3095.340609	259072.031219	53.663745
3095.120919	258900.745783	53.668749
3093.874574	258747.908641	53.673754
3093.620553	258589.668240	53.678759
3093.235380	258436.516733	53.683764
3092.291717	258276.475610	53.688769
3091.674028	258111.009365	53.693773
3090.767130	257954.375281	53.698778
3090.547990	257794.219820	53.703783
3089.321893	257637.178048	53.708788
3089.006848	257489.695289	53.713793
3088.582035	257321.193920	53.718797
3087.659593	257160.488046	53.723802
3087.296598	256999.540945	53.728807
3086.159079	256842.867712	53.733812
3085.591795	256681.545692	53.738817
3084.989502	256519.210639	53.743821
3084.170263	256363.735274	53.748826
3083.920102	256203.458512	53.753831
3082.852088	256049.015968	53.758836
3082.399982	255894.246858	53.763841
3081.765137	255736.628984	53.768845
3080.908115	255574.946172	53.773850
3080.355972	255408.325537	53.778855
3079.415803	255261.376158	53.783860
3078.731657	255094.878536	53.788865
3077.919510	254955.752995	53.793869
3077.207558	254803.114129	53.798874
3077.118914	254638.891078	53.803879
3076.153570	254482.981838	53.808884
3075.610634	254327.591611	53.813889
3075.389613	254172.226962	53.818893
3074.419361	254015.605794	53.823898
3074.121661	253849.455530	53.828903
3073.104963	253695.337738	53.833908
3072.273328	253531.742549	53.838913
3072.078550	253378.742814	53.843917
3071.255930	253221.615064	53.848922
3070.734660	253056.061153	53.853927
3069.504543	252899.762176	53.858932
3068.922616	252743.157011	53.863937
3068.368751	252579.238566	53.868941
3067.809153	252430.295646	53.873946
3067.041351	252266.207610	53.878951
3066.199831	252105.085535	53.883956
3065.964481	251949.470347	53.888961
3065.224169	251787.746809	53.893965
3064.269468	251634.716019	53.898970
3063.873230	251472.097918	53.903975
3062.901237	251314.486152	53.908980
3062.277432	251157.277824	53.913985
3061.448030	251001.732041	53.918989
3060.786645	250848.680998	53.923994
3060.059692	250704.477359	53.928999
3059.327612	250556.734811	53.934004
3059.256732	250396.434635	53.939009
3058.367634	250236.467846	53.944013
3057.545481	250086.320662	53.949018
3057.169248	249923.599033	53.954023
3056.326241	249766.095653	53.959028
3055.616319	249606.814186	53.964033
3055.308216	249443.318268	53.969037
3054.444964	249287.601209	53.974042
3053.917918	249131.550962	53.979047
3053.235875	248981.586371	53.984052
3052.525542	248810.387564	53.989057
3052.072005	248661.125637	53.994061
3051.103015	248512.938618	53.999066
3050.539820	248350.095409	54.004071
3049.691702	248188.468911	54.009076
3048.992390	248037.056407	54.014081
3048.480441	247874.511192	54.019085
3047.834492	247727.725380	54.024090
3047.183824	247574.268361	54.029095
3046.430074	247420.522225	54.034100
3045.753387	247262.511235	54.039105
3045.255369	247092.706872	54.044109
3044.226610	246955.353887	54.049114
3043.881591	246795.686556	54.054119
3043.306944	246643.338984	54.059124
3042.481957	246485.708837	54.064129
3041.646875	246329.557479	54.069133
3041.374628	246170.872495	54.074138
3040.547227	246013.778037	54.079143
3039.716443	245868.729577	54.084148
3038.744703	245712.294947	54.089153
3038.753173	245553.719027	54.094157
3037.804537	245410.676022	54.099162
3037.224177	245245.037812	54.104167
3036.432040	245094.254288	54.109172
3035.564953	244948.957889	54.114177
3035.218307	244777.349784	54.119181
3034.114636	244634.866912	54.124186
3033.811560	244478.939037	54.129191
3032.711252	244332.636137	54.134196
3032.373760	244174.192989	54.139201
3031.893299	244018.726643	54.144205
3030.967574	243878.126324	54.149210
3030.376680	243718.450568	54.154215
3029.628530	243564.555053	54.159220
3028.945963	243420.631721	54.164225
3028.462786	243262.390998	54.169229
3027.602640	243121.119028	54.174234
3027.267663	242957.634860	54.179239
3026.298317	242810.294346	54.184244
3025.736386	242659.553589	54.189249
3025.190980	242510.796673	54.194253
3024.292425	242361.153625	54.199258
3023.887140	242208.707924	54.204263
3023.129632	242053.975384	54.209268
3022.299295	241909.695195	54.214273
3021.714257	241747.499976	54.219277
3021.063534	241596.239804	54.224282
3020.504744	241442.036810	54.229287
3020.000240	241285.380798	54.234292
3019.052428	241135.034031	54.239297
3018.806403	240974.415933	54.244301
3017.860277	240831.581383	54.249306
3017.057458	240676.450341	54.254311
3016.369517	240535.128628	54.259316
3015.754074	240385.748786	54.264321
3015.200057	240231.266493	54.269325
3014.404593	240083.239691	54.274330
3014.033670	239932.191993	54.279335
3012.978192	239772.900494	54.284340
3012.361254	239623.929299	54.289345
3011.854087	239472.623659	54.294349
3010.946860	239314.913588	54.299354
3010.534368	239169.068209	54.304359
3010.100817	239020.578060	54.309364
3009.497693	238875.832735	54.314369
3008.829732	238719.384300	54.319373
3008.077307	238557.729288	54.324378
3007.130435	238407.360460	54.329383
3006.497768	238241.434432	54.334388
3005.908133	238086.960691	54.339393
3005.176373	237946.795013	54.344397
3004.427464	237795.555369	54.349402
3003.742698	237635.087809	54.354407
3002.757139	237493.129480	54.359412
3002.143406	237355.721453	54.364417
3001.713395	237202.547823	54.369421
3000.986923	237056.296585	54.374426
3000.402740	236905.541388	54.379431
2999.563941	236756.736493	54.384436
2998.905933	236606.655464	54.389441
2998.500775	236454.166496	54.394445
2997.967508	236311.094130	54.399450
2997.161937	236165.365915	54.404455
2996.367584	236012.073432	54.409460
2995.630049	235861.904202	54.414465
2994.987379	235722.542180	54.419469
2994.301471	235589.018335	54.424474
2993.801567	235431.860572	54.429479
2993.005461	235291.937761	54.434484
2992.124611	235145.993728	54.439489
2991.704215	234997.787166	54.444493
2990.887530	234843.837911	54.449498
2990.011116	234700.618393	54.454503
2989.926736	234559.030665	54.459508
2988.913933	234404.502008	54.464513
2988.374115	234264.514584	54.469517
2987.550478	234124.903306	54.474522
2986.719354	233971.517866	54.479527
2986.166968	233841.794661	54.484532
2985.577778	233708.792719	54.489537
2985.378812	233551.131922	54.494541
2984.421773	233405.762678	54.499546
2984.001148	233254.808743	54.504551
2983.329932	233117.339115	54.509556
2982.157084	232971.724590	54.514561
2981.920379	232817.864918	54.519565
2981.362838	232680.912635	54.524570
2980.694320	232524.931989	54.529575
2980.064085	232381.931511	54.534580
2979.189346	232234.412136	54.539585
2978.624557	232089.619351	54.544589
2977.779007	231941.230083	54.549594
2977.236096	231775.860555	54.554599
2976.509728	231636.593950	54.559604
2975.665442	231495.105522	54.564609
2975.332429	231353.409060	54.569613
2974.600234	231204.773852	54.574618
2974.080606	231069.472958	54.579623
2973.121902	230919.855571	54.584628
2972.498536	230773.419048	54.589633
2971.907095	230613.788277	54.594637
2971.115912	230471.656453	54.599642
2970.507503	230326.440461	54.604647
2969.838089	230185.104596	54.609652
2969.498992	230035.696113	54.614657
2969.020519	229884.553063	54.619661
2967.945413	229744.300591	54.624666
2967.427373	229584.660011	54.629671
2966.646807	229447.213112	54.634676
2965.722250	229292.424242	54.639681
2965.228678	229147.853980	54.644685
2964.530527	229004.258426	54.649690
2964.179341	228860.633638	54.654695
2962.903206	228714.787577	54.659700
2962.662266	228568.676031	54.664705
2962.254730	228424.398875	54.669709
2961.185840	228281.728887	54.674714
2960.408698	228134.760875	54.679719
2960.070336	227997.475390	54.684724
2959.015588	227845.968753	54.689729
2958.867232	227695.872034	54.694733
2957.903740	227549.927513	54.699738
2957.143907	227403.772770	54.704743
2956.722705	227271.441048	54.709748
2956.116679	227125.873502	54.714753
2955.728532	226978.005669	54.719757
2954.425490	226822.822825	54.724762
2954.105257	226671.914903	54.729767
2953.331606	226521.613714	54.734772
2952.701115	226391.162428	54.739777
2952.003185	226239.182064	54.744781
2951.530411	226099.616709	54.749786
2950.696981	225951.999403	54.754791
2950.185817	225809.067052	54.759796
2949.335763	225659.021394	54.764801
2948.925732	225521.114761	54.769805
2947.999570	225382.157070	54.774810
2947.453293	225221.485209	54.779815
2946.997518	225080.684047	54.784820
2945.969568	224936.472890	54.789825
2945.517055	224799.528970	54.794829
2944.594387	224643.386155	54.799834
2944.140068	224500.396172	54.804839
2943.436831	224355.281721	54.809844
2942.398999	224213.530344	54.814849
2941.998138	224062.398109	54.819853
2940.812825	223936.277714	54.824858
2940.591334	223780.878489	54.829863
2939.971865	223643.250090	54.834868
2939.046884	223507.630725	54.839873
2938.727598	223365.410661	54.844877
2937.968718	223228.046927	54.849882
2937.670153	223077.040406	54.854887
2936.577547	222930.449881	54.859892
2936.077755	222795.502768	54.864897
2935.424516	222643.776710	54.869901
2934.718257	222503.949049	54.874906
2933.801874	222364.154907	54.879911
2933.365364	222218.111076	54.884916
2932.425919	222080.625199	54.889921
2931.894116	221934.558803	54.894925
2931.335660	221801.252126	54.899930
2930.830273	221660.375814	54.904935
2929.874487	221512.518809	54.909940
2929.073710	221372.797281	54.914945
2928.693489	221238.814156	54.919949
2927.770084	221094.033420	54.924954
2927.377395	220948.812508	54.929959
2926.666935	220810.401602	54.934964
2925.800564	220670.895434	54.939969
2925.423571	220525.761962	54.944973
2924.360690	220390.806418	54.949978
2924.109773	220248.033947	54.954983
2923.297580	220113.739339	54.959988
2922.539239	219976.966934	54.964993
2922.212200	219826.480548	54.969997
2921.366487	219690.257144	54.975002
2920.653615	219549.277630	54.980007
2920.219015	219411.092977	54.985012
2919.246727	219278.951042	54.990017
2918.906344	219128.608222	54.995021
2917.930935	218986.143845	55.000026
2917.316006	218838.683723	55.005031
2916.686203	218698.698314	55.010036
2915.605745	218586.725142	55.015041
2915.324681	218431.906423	55.020045
2914.387729	218299.646118	55.025050
2913.854667	218168.174963	55.030055
2913.232145	218027.858750	55.035060
2912.854634	217880.439377	55.040065
2912.225718	217748.564111	55.045069
2911.076892	217619.075363	55.050074
2910.604812	217470.564387	55.055079
2910.392168	217341.424353	55.060084
2909.200843	217195.369968	55.065089
2908.901770	217045.266833	55.070093
2907.999671	216918.031517	55.075098
2907.366549	216773.735322	55.080103
2906.599575	216635.761404	55.085108
2906.249634	216499.338292	55.090113
2905.501545	216362.265673	55.095117
2904.358756	216230.003658	55.100122
2903.827851	216090.313247	55.105127
2903.487223	215958.624823	55.110132
2902.504223	215825.969149	55.115137
2902.308938	215673.064956	55.120141
2901.528635	215537.131931	55.125146
2900.627068	215401.014720	55.130151
2899.768597	215270.542459	55.135156
2899.233948	215140.324661	55.140161
2898.670423	214997.994097	55.145165
2897.996253	214875.168735	55.150170
2897.464166	214727.271392	55.155175
2896.969423	214587.451045	55.160180
2895.972936	214450.828904	55.165185
2895.413764	214314.481466	55.170189
2894.649210	214181.119814	55.175194
2894.033335	214033.402734	55.180199
2893.201523	213911.571452	55.185204
2892.522292	213770.725569	55.190209
2892.309923	213626.165768	55.195213
2891.501361	213506.788109	55.200218
2891.033290	213359.863733	55.205223
2890.352585	213219.388375	55.210228
2889.352131	213081.955071	55.215233
2889.155316	212942.714689	55.220237
2888.450078	212796.745551	55.225242
2887.779665	212665.179447	55.230247
2886.778974	212528.765592	55.235252
2885.956008	212389.841910	55.240257
2885.531275	212246.960691	55.245261
2884.656557	212108.631295	55.250266
2884.124971	211977.019147	55.255271
2883.929385	211840.326524	55.260276
2882.732128	211709.303988	55.265281
2882.230978	211559.206931	55.270285
2881.294260	211433.260319	55.275290
2880.697652	211290.981190	55.280295
2880.262767	211155.982535	55.285300
2879.555635	211011.710534	55.290305
2878.957411	210881.307601	55.295309
2877.817168	210754.350884	55.300314
2877.673273	210614.674407	55.305319
2876.652308	210477.097181	55.310324
2876.039288	210339.010192	55.315329
2875.783459	210199.479635	55.320333
2874.823395	210071.324823	55.325338
2874.087721	209937.712797	55.330343
2873.326573	209808.814282	55.335348
2872.782155	209669.737884	55.340353
2872.362453	209527.472904	55.345357
2871.534238	209394.143975	55.350362
2870.960139	209271.809778	55.355367
2870.429147	209128.099682	55.360372
2869.335876	208989.086265	55.365377
2869.117158	208849.209220	55.370381
2868.282050	208718.199220	55.375386
2867.319037	208576.404283	55.380391
2866.904276	208456.808297	55.385396
2866.159461	208321.432123	55.390401
2865.664385	208173.544041	55.395405
2864.626494	208038.545812	55.400410
2864.077371	207909.172250	55.405415
2863.528614	207775.484412	55.410420
2862.566254	207639.660576	55.415425
2862.124231	207514.330843	55.420429
2861.396856	207388.346568	55.425434
2860.587530	207246.594039	55.430439
2859.791518	207123.586582	55.435444
2859.011944	206992.622426	55.440449
2858.954918	206860.691436	55.445453
2857.659618	206741.785539	55.450458
2857.191075	206609.602096	55.455463
2856.544165	206480.348913	55.460468
2855.874584	206358.468431	55.465473
2855.327319	206225.089262	55.470477
2854.376140	206106.308322	55.475482
2853.968558	205963.986159	55.480487
2853.580315	205837.544209	55.485492
2852.530978	205708.750969	55.490497
2851.819186	205590.620403	55.495501
2851.509171	205465.515892	55.500506
2850.431761	205330.339162	55.505511
2850.048068	205199.532645	55.510516
2849.273084	205067.986611	55.515521
2849.108595	204937.629579	55.520525
2848.321178	204821.166994	55.525530
2847.928765	204679.112814	55.530535
2847.286563	204544.059893	55.535540
2846.197958	204411.470542	55.540545
2846.226626	204271.450538	55.545549
2845.312762	204138.910502	55.550554
2844.459634	204004.083145	55.555559
2843.911699	203869.920448	55.560564
2843.068921	203727.583600	55.565569
2842.402356	203593.720314	55.570573
2841.422892	203466.499059	55.575578
2840.792012	203328.151130	55.580583
2840.195387	203195.003099	55.585588
2839.324122	203080.809857	55.590593
2838.971895	202934.388592	55.595597
2838.085567	202811.659088	55.600602
2837.621538	202683.428970	55.605607
2837.070685	202547.462769	55.610612
2836.409053	202419.353627	55.615617
2835.717956	202275.660189	55.620621
2835.152404	202153.823045	55.625626
2834.455088	202018.937571	55.630631
2833.799035	201885.534811	55.635636
2832.704097	201752.685454	55.640641
2832.542193	201619.714110	55.645645
2831.490940	201485.942219	55.650650
2830.842726	201360.136749	55.655655
2830.332113	201237.911142	55.660660
2829.611434	201105.843966	55.665665
2829.045132	200971.385694	55.670669
2828.203298	200847.228212	55.675674
2827.620073	200702.032880	55.680679
2826.750838	200585.528392	55.685684
2825.785986	200459.571520	55.690689
2825.668828	200320.933380	55.695693
2824.691714	200197.256915	55.700698
2824.155147	200070.482317	55.705703
2823.673358	199959.211583	55.710708
2823.253002	199814.463663	55.715713
2822.355914	199686.881733	55.720717
2821.498950	199559.370102	55.725722
2821.101470	199425.143420	55.730727
2820.483486	199300.674068	55.735732
2819.724460	199174.102232	55.740737
2819.239285	199040.386682	55.745741
2818.328721	198918.840439	55.750746
2817.872310	198781.074387	55.755751
2817.246874	198657.256692	55.760756
2816.539455	198523.412206	55.765761
2816.007288	198385.010198	55.770765
2815.091875	198253.909758	55.775770
2814.521562	198113.720277	55.780775
2813.667973	197990.589242	55.785780
2813.133881	197862.025268	55.790785
2812.678353	197728.600995	55.795789
2811.950807	197601.455303	55.800794
2811.353389	197462.836998	55.805799
2810.562306	197329.721376	55.810804
2809.553513	197208.436394	55.815809
2809.259395	197080.765233	55.820813
2808.465169	196954.942316	55.825818
2807.958723	196815.891404	55.830823
2807.335824	196683.921461	55.835828
2806.439955	196551.536999	55.840833
2805.982084	196413.548336	55.845837
2805.282769	196293.247164	55.850842
2804.697310	196155.381192	55.855847
2803.845697	196025.599585	55.860852
2803.206486	195892.030967	55.865857
2802.884456	195755.244093	55.870861
2802.098201	195630.581055	55.875866
2800.931722	195497.415078	55.880871
2800.623305	195359.456469	55.885876
2799.546502	195233.453469	55.890881
2799.301053	195105.474104	55.895885
2798.495696	194975.916869	55.900890
2797.926294	194847.645907	55.905895
2797.088829	194717.827209	55.910900
2796.411399	194589.535836	55.915905
2796.038599	194459.453348	55.920909
2794.891443	194335.359606	55.925914
2794.489715	194204.582535	55.930919
2794.166205	194076.350930	55.935924
2793.258785	193947.817689	55.940929
2792.813481	193814.707333	55.945933
2792.026644	193678.483183	55.950938
2791.239681	193551.865906	55.955943
2790.595774	193425.518940	55.960948
2789.835148	193292.879799	55.965953
2789.777979	193158.144698	55.970957
2788.621363	193033.419501	55.975962
2787.822944	192897.224770	55.980967
2787.474174	192773.428344	55.985972
2786.415562	192645.125990	55.990977
2785.847800	192515.715622	55.995981
2785.190991	192401.435240	56.000986
2784.576517	192255.632333	56.005991
2783.707643	192123.369732	56.010996
2782.911138	192001.885485	56.016001
2782.759233	191875.858983	56.021005
2781.811542	191757.045754	56.026010
2781.181269	191622.036642	56.031015
2781.039327	191491.581837	56.036020
2780.058955	191364.606391	56.041025
2779.448695	191225.002116	56.046029
2778.597664	191102.765352	56.051034
2778.267113	190975.242692	56.056039
2777.467299	190845.657208	56.061044
2776.561645	190720.910884	56.066049
2776.317150	190582.166593	56.071053
2775.424588	190454.530753	56.076058
2774.522963	190323.703220	56.081063
2774.062980	190186.610018	56.086068
2773.153593	190073.202111	56.091073
2772.827807	189935.350445	56.096077
2771.700342	189818.122652	56.101082
2771.414539	189679.273009	56.106087
2770.949656	189562.793328	56.111092
2769.970910	189419.054146	56.116097
2769.470796	189295.761311	56.121101
2768.543046	189174.483098	56.126106
2768.232863	189046.249877	56.131111
2767.685979	188916.069767	56.136116
2766.951066	188790.474478	56.141121
2766.267831	188645.533086	56.146125
2765.513604	188519.114615	56.151130
2764.766728	188379.056841	56.156135
2764.350503	188256.618561	56.161140
2763.348380	188133.331943	56.166145
2762.870595	187997.571024	56.171149
2762.069720	187856.581911	56.176154
2761.335577	187742.413950	56.181159
2760.691569	187606.438774	56.186164
2760.062050	187485.512079	56.191169
2759.665052	187352.780852	56.196173
2758.930501	187229.848633	56.201178
2758.674919	187097.312014	56.206183
2757.837735	186963.722909	56.211188
2756.699830	186831.797522	56.216193
2756.203077	186696.603180	56.221197
2755.351461	186570.485316	56.226202
2754.874720	186449.498968	56.231207
2754.210263	186313.836159	56.236212
2753.155947	186191.377184	56.241217
2752.675597	186058.942765	56.246221
2751.896729	185939.265080	56.251226
2751.719762	185805.523884	56.256231
2751.033870	185679.165956	56.261236
2750.105372	185554.220750	56.266241
2749.717762	185416.099638	56.271245
2748.861026	185289.032001	56.276250
2748.500093	185163.794423	56.281255
2747.801823	185031.766438	56.286260
2746.978674	184909.007150	56.291265
2746.719858	184772.012537	56.296269
2745.806220	184639.650891	56.301274
2744.859013	184502.359053	56.306279
2744.335668	184375.559216	56.311284
2743.653583	184255.412687	56.316289
2742.995643	184114.361593	56.321293
2742.214871	183997.666133	56.326298
2741.478223	183871.804718	56.331303
2741.068645	183739.429496	56.336308
2740.342525	183602.016354	56.341313
2739.738983	183468.858508	56.346317
2738.786488	183354.697990	56.351322
2738.287761	183211.958075	56.356327
2737.736734	183089.529590	56.361332
2736.915169	182964.472899	56.366337
2736.580613	182830.053154	56.371341
2735.572914	182708.664852	56.376346
2735.053679	182575.076553	56.381351
2734.396342	182446.980478	56.386356
2734.094471	182320.100547	56.391361
2733.385671	182180.335744	56.396365
2732.302491	182057.371110	56.401370
2731.715506	181926.148846	56.406375
2731.128767	181797.063999	56.411380
2730.270405	181660.123086	56.416385
2729.658885	181525.967460	56.421389
2729.081108	181407.771124	56.426394
2728.231980	181276.923074	56.431399
2727.661950	181148.880582	56.436404
2726.916903	181021.464050	56.441409
2726.893666	180889.964807	56.446413
2725.692538	180763.995077	56.451418
2725.194953	180627.763496	56.456423
2724.682301	180503.707991	56.461428
2723.517635	180382.707213	56.466433
2723.123912	180250.861560	56.471437
2722.319416	180114.514860	56.476442
2721.949570	179991.633904	56.481447
2721.345548	179861.857974	56.486452
2720.561332	179734.922102	56.491457
2719.784952	179597.376918	56.496461
2718.712912	179486.552695	56.501466
2718.087187	179352.698656	56.506471
2717.888119	179221.830215	56.511476
2717.058774	179099.368057	56.516481
2716.543737	178967.698225	56.521485
2715.962256	178838.913988	56.526490
2715.410229	178709.387734	56.531495
2714.482077	178584.335182	56.536500
2713.780510	178454.477251	56.541505
2713.659062	178321.983906	56.546509
2712.741850	178199.182131	56.551514
2712.064766	178056.691046	56.556519
2711.535704	177921.859549	56.561524
2710.637879	177797.287876	56.566529
2709.857543	177671.476902	56.571533
2709.345403	177536.720282	56.576538
2708.717212	177396.653095	56.581543
2708.151695	177268.189133	56.586548
2707.501128	177140.095178	56.591553
2706.877278	177004.747454	56.596557
2706.009812	176879.359692	56.601562
2705.270253	176748.851688	56.606567
2704.820924	176611.099131	56.611572
2704.086157	176477.729437	56.616577
2703.680647	176342.540076	56.621581
2702.855058	176210.775504	56.626586
2702.095252	176082.142500	56.631591
2701.537329	175953.503355	56.636596
2700.640551	175823.697288	56.641601
2700.189850	175682.412227	56.646605
2699.445255	175550.815007	56.651610
2698.489638	175426.196046	56.656615
2698.263326	175286.530236	56.661620
2697.460458	175156.749566	56.666625
2696.966879	175029.057033	56.671629
2696.214459	174901.825618	56.676634
2695.658631	174766.296441	56.681639
2694.958086	174630.676177	56.686644
2694.077438	174498.442557	56.691649
2693.674088	174356.277029	56.696653
2692.984887	174230.436728	56.701658
2692.271155	174095.392674	56.706663
2691.484169	173960.411551	56.711668
2690.960481	173834.508111	56.716673
2690.090941	173698.650672	56.721677
2689.756237	173575.338045	56.726682
2688.888272	173445.255238	56.731687
2688.238605	173305.307236	56.736692
2687.440104	173179.042416	56.741697
2687.222186	173038.607258	56.746701
2686.376431	172908.115708	56.751706
2685.789552	172776.464403	56.756711
2685.261260	172623.107669	56.761716
2684.421147	172494.117286	56.766721
2684.005841	172360.723280	56.771725
2683.108544	172232.531307	56.776730
2682.457348	172081.790546	56.781735
2681.705237	171946.085817	56.786740
2680.725599	171814.207429	56.791745
2680.379134	171681.186339	56.796749
2679.893595	171556.466798	56.801754
2679.202883	171430.533850	56.806759
2678.526943	171285.357572	56.811764
2677.667169	171162.415418	56.816769
2677.421046	171007.723096	56.821773
2676.490711	170885.797656	56.826778
2675.792952	170748.638694	56.831783
2675.143873	170602.901139	56.836788
2674.586803	170486.958461	56.841793
2674.119405	170337.924816	56.846797
2673.380099	170206.713217	56.851802
2672.397875	170065.697605	56.856807
2671.840436	169926.522749	56.861812
2671.130695	169795.028088	56.866817
2670.822488	169657.353459	56.871821
2669.796879	169523.201080	56.876826
2669.188120	169388.487174	56.881831
2668.810398	169242.101348	56.886836
2667.857793	169113.915683	56.891841
2667.222797	168973.853672	56.896845
2666.468787	168849.948361	56.901850
2665.874611	168705.697110	56.906855
2664.940235	168570.605303	56.911860
2664.395240	168438.949304	56.916865
2663.718890	168295.780802	56.921869
2662.894327	168174.165097	56.926874
2662.643274	168047.054486	56.931879
2662.362071	167897.326846	56.936884
2661.255753	167769.653272	56.941889
2660.918011	167620.380749	56.946893
2660.403254	167484.921133	56.951898
2659.373475	167352.837062	56.956903
2658.846944	167202.019309	56.961908
2658.153319	167071.917528	56.966913
2657.691599	166928.173405	56.971917
2656.728261	166796.335079	56.976922
2656.186524	166657.296832	56.981927
2655.891889	166516.045550	56.986932
2654.712484	166372.633429	56.991937
2654.150666	166228.322923	56.996941
2653.463517	166100.982792	57.001946
2652.754258	165950.758508	57.006951
2652.440056	165810.975285	57.011956
2651.541664	165670.395059	57.016961
2651.107395	165530.212302	57.021965
2650.430439	165397.481610	57.026970
2649.682170	165249.377101	57.031975
2649.192088	165104.805280	57.036980
2648.215209	164972.911979	57.041985
2647.579517	164822.795046	57.046989
2646.918244	164685.753967	57.051994
2646.464356	164537.109782	57.056999
2645.828366	164399.989470	57.062004
2644.863213	164271.046722	57.067009
2644.454530	164116.573596	57.072013
2643.623902	163979.918002	57.077018
2643.077875	163847.477310	57.082023
2642.688051	163685.742819	57.087028
2641.758192	163557.242014	57.092033
2641.096651	163403.117119	57.097037
2640.090756	163272.060995	57.102042
2639.761575	163128.094493	57.107047
2639.192858	162984.954817	57.112052
2638.037261	162858.971591	57.117057
2637.549425	162704.809423	57.122061
2637.006186	162575.081107	57.127066
2636.213511	162441.769178	57.132071
2636.112024	162294.883745	57.137076
2635.017295	162153.775996	57.142081
2634.405501	162005.777454	57.147085
2633.752917	161869.470317	57.152090
2632.963224	161726.663070	57.157095
2632.355958	161591.239799	57.162100
2631.399542	161451.104597	57.167105
2631.298249	161305.189445	57.172109
2630.250818	161159.513797	57.177114
2629.616116	161024.338585	57.182119
2629.178320	160872.096151	57.187124
2628.312220	160741.116100	57.192129
2627.763542	160605.916133	57.197133
2627.264386	160467.098147	57.202138
2626.640329	160326.469732	57.207143
2625.800911	160174.510055	57.212148
2624.924536	160047.233849	57.217153
2624.713225	159904.532973	57.222157
2623.842792	159766.386811	57.227162
2622.949387	159618.582662	57.232167
2622.265362	159477.395027	57.237172
2621.727953	159333.934478	57.242177
2621.337128	159191.379355	57.247181
2620.690289	159059.010490	57.252186
2619.894963	158924.873101	57.257191
2619.294811	158781.284911	57.262196
2618.580141	158639.584271	57.267201
2617.968057	158487.150916	57.272205
2617.233392	158348.823562	57.277210
2616.235529	158207.156839	57.282215
2615.931616	158067.618192	57.287220
2615.290152	157920.887315	57.292225
2614.662535	157789.511820	57.297229
2613.950270	157645.462997	57.302234
2613.151625	157503.271790	57.307239
2612.854961	157352.763891	57.312244
2611.968224	157216.905961	57.317249
2611.575005	157075.529437	57.322253
2610.881805	156939.578371	57.327258
2609.956277	156789.236140	57.332263
2609.451960	156638.319333	57.337268
2608.804486	156500.125399	57.342273
2608.161115	156350.083614	57.347277
2607.434805	156203.576888	57.352282
2606.733042	156063.728029	57.357287
2606.278989	155914.967499	57.362292
2605.176879	155772.933241	57.367297
2604.726344	155622.609857	57.372301
2604.280739	155488.621096	57.377306
2603.565910	155351.688248	57.382311
2602.943777	155208.970124	57.387316
2602.118276	155061.238281	57.392321
2601.554544	154907.707227	57.397325
2600.848250	154758.495977	57.402330
2600.138300	154619.213674	57.407335
2599.900315	154465.035572	57.412340
2599.060883	154322.787814	57.417345
2598.353786	154174.189426	57.422349
2597.421319	154025.118954	57.427354
2596.914913	153874.952020	57.432359
2596.881430	153663.951342	57.437364
2595.773614	153531.320984	57.442369
2595.080557	153380.270644	57.447373
2594.355238	153232.391141	57.452378
2593.857837	153086.764149	57.457383
2593.060144	152930.190452	57.462388
2592.091859	152789.736447	57.467393
2591.822726	152637.694406	57.472397
2590.908428	152488.729606	57.477402
2590.067019	152357.091286	57.482407
2589.655432	152209.852996	57.487412
2588.462251	152056.994040	57.492417
2588.631083	151908.953323	57.497421
2587.800822	151788.005040	57.502426
2587.259672	151623.541807	57.507431
2586.812771	151468.457397	57.512436
2585.962806	151324.152354	57.517441
2585.090849	151175.606216	57.522445
2584.686269	151020.911230	57.527450
2583.926317	150876.136329	57.532455
2583.178726	150723.912022	57.537460
2582.370486	150573.413884	57.542465
2581.915954	150412.387409	57.547469
2581.250369	150269.938869	57.552474
2580.415776	150136.846740	57.557479
2579.873872	149955.424409	57.562484
2579.275189	149824.342446	57.567489
2578.681820	149680.830140	57.572493
2577.929726	149529.844969	57.577498
2577.296570	149382.756188	57.582503
2576.868230	149232.801409	57.587508
2575.945023	149060.569912	57.592513
2575.400827	148918.972316	57.597517
2575.055668	148775.119676	57.602522
2574.080254	148619.395466	57.607527
2573.525258	148453.476189	57.612532
2572.405658	148305.846666	57.617537
2572.009536	148155.319894	57.622541
2571.264748	148030.902499	57.627546
2570.658109	147859.974430	57.632551
2569.867963	147716.006427	57.637556
2569.392345	147563.220155	57.642561
2568.764117	147414.373093	57.647565
2568.239065	147253.843807	57.652570
2567.184079	147106.692525	57.657575
2566.814818	146953.066269	57.662580
2565.960454	146805.007704	57.667585
2565.387694	146656.676453	57.672589
2564.884492	146496.249207	57.677594
2563.979459	146347.972062	57.682599
2563.336108	146200.797886	57.687604
2562.830360	146059.270448	57.692609
2562.301349	145904.785031	57.697613
2561.488904	145746.482034	57.702618
2560.795716	145602.838690	57.707623
2560.288038	145432.950101	57.712628
2559.429815	145290.185777	57.717633
2558.752923	145141.280902	57.722637
2558.033858	144990.540794	57.727642
2557.335651	144838.883153	57.732647
2557.011431	144687.815072	57.737652
2556.350050	144531.082743	57.742657
2555.849209	144369.649397	57.747661
2555.081491	144219.403616	57.752666
2554.369827	144068.755751	57.757671
2553.991002	143902.146299	57.762676
2552.973257	143761.371198	57.767681
2552.285877	143592.105667	57.772685
2551.738498	143437.355831	57.777690
2550.934339	143284.769546	57.782695
2550.447988	143124.585690	57.787700
2549.264978	142993.230764	57.792705
2548.895373	142818.315359	57.797709
2548.377732	142671.747889	57.802714
2547.521873	142523.659082	57.807719
2547.029419	142367.736904	57.812724
2546.275686	142212.670152	57.817729
2545.843791	142062.661219	57.822733
2544.827303	141903.813002	57.827738
2544.156020	141747.795264	57.832743
2543.748347	141598.661519	57.837748
2542.944343	141451.560794	57.842753
2542.582568	141279.842236	57.847757
2541.715433	141137.009630	57.852762
2540.791281	140982.293810	57.857767
2540.304977	140828.995997	57.862772
2539.678738	140688.655831	57.867777
2538.967115	140532.460148	57.872781
2538.350059	140371.333119	57.877786
2537.651502	140223.522831	57.882791
2537.053141	140058.493835	57.887796
2536.356985	139919.578666	57.892801
2536.030185	139767.518832	57.897805
2535.065947	139604.125813	57.902810
2534.085910	139455.919219	57.907815
2534.078952	139289.365006	57.912820
2533.282765	139139.288561	57.917825
2532.614984	138985.584223	57.922829
2531.720328	138831.357605	57.927834
2531.096463	138659.327093	57.932839
2530.845452	138522.660199	57.937844
2529.764630	138356.954754	57.942849
2529.076684	138206.294132	57.947853
2528.690380	138044.279136	57.952858
2527.711728	137894.682561	57.957863
2527.239804	137733.457828	57.962868
2526.400831	137580.054698	57.967873
2525.954782	137425.954861	57.972877
2525.361183	137263.824540	57.977882
2524.611675	137110.714581	57.982887
2524.236227	136951.054187	57.987892
2523.156609	136801.771363	57.992897
2522.781496	136642.862146	57.997901
2521.991163	136494.678419	58.002906
2521.374519	136329.317338	58.007911
2520.988371	136173.994977	58.012916
2520.153249	136015.454267	58.017921
2519.456697	135844.125017	58.022925
2518.867344	135691.263878	58.027930
2517.929733	135531.560586	58.032935
2517.790824	135369.051099	58.037940
2516.824696	135220.647634	58.042945
2515.887943	135063.423990	58.047949
2515.370414	134908.167316	58.052954
2514.489186	134745.067581	58.057959
2514.397762	134579.468057	58.062964
2513.659327	134420.958839	58.067969
2513.046139	134260.448939	58.072973
2512.491574	134099.994157	58.077978
2511.605745	133943.899117	58.082983
2511.199149	133767.670917	58.087988
2509.907336	133622.147360	58.092993
2509.655152	133447.916416	58.097997
2508.937285	133292.712904	58.103002
2508.233677	133144.075283	58.108007
2507.365495	132980.068897	58.113012
2506.712068	132820.500724	58.118017
2506.152930	132660.766069	58.123021
2505.366291	132510.290342	58.128026
2504.634545	132359.260509	58.133031
2504.276143	132192.662785	58.138036
2503.495048	132038.187453	58.143041
2502.899091	131873.559993	58.148045
2502.129058	131712.352539	58.153050
2501.556176	131557.834123	58.158055
2500.802683	131394.733256	58.163060
2500.165427	131258.911248	58.168065
2499.691663	131080.639916	58.173069
2498.976439	130922.781559	58.178074
2498.170783	130771.784619	58.183079
2497.699928	130601.009847	58.188084
2496.972474	130447.309518	58.193089
2496.225585	130289.269216	58.198093
2495.567088	130119.962378	58.203098
2494.875074	129965.776421	58.208103
2494.212395	129805.947319	58.213108
2493.457427	129644.533414	58.218113
2492.762136	129490.325200	58.223117
2492.464103	129336.829634	58.228122
2491.495250	129169.724224	58.233127
2491.339070	129015.941223	58.238132
2490.602637	128852.128511	58.243137
2489.809097	128706.017927	58.248141
2488.954945	128540.993741	58.253146
2488.431932	128382.357246	58.258151
2488.011455	128202.901985	58.263156
2486.802016	128051.844083	58.268161
2486.450287	127884.623209	58.273165
2485.677154	127733.917004	58.278170
2484.993778	127576.123380	58.283175
2484.474823	127402.607236	58.288180
2483.652882	127261.423755	58.293185
2482.887161	127095.136906	58.298189
2482.188083	126933.628368	58.303194
2481.945949	126775.578908	58.308199
2481.228616	126612.957570	58.313204
2480.374413	126459.997959	58.318209
2480.275009	126295.934394	58.323213
2479.610362	126121.077909	58.328218
2478.404901	125961.623815	58.333223
2478.193249	125796.196810	58.338228
2477.374360	125639.197810	58.343233
2476.780205	125457.045020	58.348237
2476.146843	125309.276258	58.353242
2475.234978	125136.751146	58.358247
2474.778103	124974.365005	58.363252
2473.732846	124816.263750	58.368257
2473.352977	124651.708527	58.373261
2472.682400	124486.527353	58.378266
2471.482894	124324.415226	58.383271
2471.250123	124158.480938	58.388276
2470.545730	124005.765419	58.393281
2469.947339	123831.967215	58.398285
2469.762711	123670.675945	58.403290
2468.644651	123509.711384	58.408295
2468.345805	123338.167294	58.413300
2467.387475	123179.833330	58.418305
2466.987227	123005.526555	58.423309
2466.230290	122840.496196	58.428314
2465.450615	122671.762676	58.433319
2464.553164	122511.315182	58.438324
2464.032640	122354.097627	58.443329
2463.392478	122184.837173	58.448333
2462.548931	122030.326555	58.453338
2461.907461	121863.061887	58.458343
2461.611849	121693.534096	58.463348
2460.763946	121538.138222	58.468353
2460.304293	121370.047917	58.473357
2459.706639	121195.847810	58.478362
2458.712839	121038.192513	58.483367
2458.017108	120864.340272	58.488372
2457.273647	120703.384160	58.493377
2456.477627	120546.373401	58.498381
2455.873373	120378.452019	58.503386
2455.264611	120226.124010	58.508391
2454.633849	120068.975644	58.513396
2454.070028	119924.260262	58.518401
2453.555695	119740.851584	58.523405
2452.990233	119572.357884	58.528410
2451.979086	119409.795283	58.533415
2451.594014	119244.493629	58.538420
2450.686608	119079.904288	58.543425
2450.188689	118911.061365	58.548429
2449.475526	118749.318992	58.553434
2448.767495	118592.318747	58.558439
2448.358259	118425.489929	58.563444
2447.454522	118271.645832	58.568449
2447.040837	118105.937009	58.573453
2446.607723	117931.510441	58.578458
2445.565514	117766.055783	58.583463
2444.801116	117591.912550	58.588468
2444.034882	117435.569684	58.593473
2443.478134	117272.091548	58.598477
2443.089445	117115.449569	58.603482
2441.919865	116940.987775	58.608487
2441.736951	116778.450088	58.613492
2440.751920	116620.255316	58.618497
2440.227997	116453.355904	58.623501
2439.625405	116291.814564	58.628506
2438.738480	116130.116205	58.633511
2438.377447	115962.248425	58.638516
2437.838881	115800.039930	58.643521
2436.842883	115624.112439	58.648525
2436.525769	115457.262932	58.653530
2435.629493	115306.018776	58.658535
2435.060317	115129.538319	58.663540
2434.450514	114972.087698	58.668545
2433.801647	114801.899411	58.673549
2433.145147	114637.654261	58.678554
2432.355331	114463.999752	58.683559
2431.776916	114304.047621	58.688564
2430.871203	114144.643447	58.693569
2430.286507	113964.822444	58.698573
2429.769648	113811.692860	58.703578
2428.849404	113642.431281	58.708583
2428.518108	113485.853374	58.713588
2427.885522	113326.703040	58.718593
2426.922439	113151.073180	58.723597
2426.768752	112978.076995	58.728602
2425.971752	112817.255085	58.733607
2425.227318	112648.721244	58.738612
2424.585129	112482.260313	58.743617
2424.174784	112309.760044	58.748621
2423.502887	112143.915337	58.753626
2422.437230	111964.902100	58.758631
2421.995203	111798.515551	58.763636
2421.352207	111633.932575	58.768641
2420.627679	111465.930333	58.773645
2420.034299	111293.726333	58.778650
2419.294703	111127.930884	58.783655
2418.715412	110953.778766	58.788660
2417.846133	110786.235623	58.793665
2417.269074	110619.345347	58.798669
2416.600125	110450.351232	58.803674
2415.632862	110289.331575	58.808679
2415.230158	110111.565648	58.813684
2414.463080	109958.689858	58.818689
2413.764074	109793.988436	58.823693
2413.379754	109619.021639	58.828698
2412.483435	109460.616953	58.833703
2412.022597	109285.277588	58.838708
2411.180142	109119.696022	58.843713
2410.704460	108949.970909	58.848717
2409.973431	108776.918004	58.853722
2409.145627	108621.680648	58.858727
2408.783574	108441.769308	58.863732
2408.260273	108277.925925	58.868737
2407.348467	108108.656544	58.873741
2406.739876	107938.978592	58.878746
2406.082711	107774.741043	58.883751
2405.579123	107602.935838	58.888756
2404.666310	107440.854032	58.893761
2404.238417	107256.298252	58.898765
2403.435878	107086.606269	58.903770
2402.612326	106921.874260	58.908775
2402.287346	106750.237156	58.913780
2401.321911	106589.762002	58.918785
2400.966861	106406.165614	58.923789
2400.200336	106248.852670	58.928794
2399.411406	106070.466947	58.933799
2399.098252	105914.695891	58.938804
2398.215103	105742.139332	58.943809
2397.615077	105556.437442	58.948813
2397.255528	105381.554469	58.953818
2396.674952	105205.159750	58.958823
2395.865197	105035.857759	58.963828
2395.066223	104863.985757	58.968833
2394.319748	104679.481297	58.973837
2393.954817	104514.648744	58.978842
2393.072940	104343.980044	58.983847
2392.834692	104157.908144	58.988852
2391.716027	103994.626168	58.993857
2391.034073	103808.062730	58.998861
2390.417817	103635.136566	59.003866
2389.604600	103473.649560	59.008871
2389.146420	103292.567726	59.013876
2388.214870	103118.439220	59.018881
2387.596245	102952.877465	59.023885
2387.004072	102782.256594	59.028890
2386.409773	102613.610236	59.033895
2385.821374	102438.531534	59.038900
2384.882229	102265.324065	59.043905
2383.971816	102087.983566	59.048909
2383.538698	101921.486183	59.053914
2382.811591	101759.026737	59.058919
2382.243153	101577.493505	59.063924
2381.480006	101411.508821	59.068929
2381.064813	101243.503672	59.073933
2379.988851	101074.462682	59.078938
2379.259572	100909.078838	59.083943
2378.987866	100731.247756	59.088948
2378.137594	100576.643776	59.093953
2377.744475	100393.969217	59.098957
2377.256042	100233.176233	59.103962
2376.326322	100059.552345	59.108967
2375.840943	99892.265852	59.113972
2374.960119	99721.472124	59.118977
2374.361902	99536.984677	59.123981
2373.728704	99365.494648	59.128986
2373.210405	99205.595228	59.133991
2372.648590	99029.110849	59.138996
2371.787580	98860.216887	59.144001
2371.301310	98686.812117	59.149005
2370.874364	98517.300032	59.154010
2369.951864	98333.444507	59.159015
2369.164277	98163.985876	59.164020
2368.591370	97998.090711	59.169025
2368.024219	97817.227437	59.174029
2367.507186	97639.199084	59.179034
2366.519912	97461.633571	59.184039
2366.017282	97294.926885	59.189044
2365.377913	97120.359563	59.194049
2364.510694	96940.330937	59.199053
2364.270554	96766.629006	59.204058
2363.014171	96589.271535	59.209063
2362.636169	96412.543577	59.214068
2361.937822	96237.351842	59.219073
2361.329039	96068.990338	59.224077
2360.660309	95890.194312	59.229082
2360.076960	95717.062212	59.234087
2359.671184	95543.053469	59.239092
2358.607191	95371.192515	59.244097
2357.881052	95193.768273	59.249101
2357.778864	95026.107930	59.254106
2356.717031	94849.126484	59.259111
2356.328957	94667.695565	59.264116
2355.374305	94499.609915	59.269121
2354.991212	94315.016597	59.274125
2354.437058	94138.328077	59.279130
2353.544008	93964.440542	59.284135
2352.842426	93776.116323	59.289140
2351.924054	93597.485951	59.294145
2351.197574	93426.899065	59.299149
2350.876505	93248.988463	59.304154
2350.024007	93076.832588	59.309159
2349.376054	92892.293042	59.314164
2348.821188	92720.479545	59.319169
2348.042818	92547.916529	59.324173
2347.388863	92362.488253	59.329178
2346.656975	92208.892797	59.334183
2346.190289	92017.876695	59.339188
2345.250439	91855.623293	59.344193
2344.422397	91685.230778	59.349197
2344.017730	91491.514553	59.354202
2343.292413	91336.123356	59.359207
2342.972552	91165.800114	59.364212
2342.142761	90995.584412	59.369217
2341.506807	90810.438980	59.374221
2341.014086	90626.407348	59.379226
2340.110143	90467.316067	59.384231
2339.596574	90289.256943	59.389236
2338.835308	90109.628095	59.394241
2338.094190	89928.856275	59.399245
2337.358613	89755.319297	59.404250
2336.740976	89587.464839	59.409255
2335.930882	89419.350545	59.414260
2335.477311	89253.539534	59.419265
2334.752472	89075.010271	59.424269
2334.136875	88892.838673	59.429274
2333.352247	88739.916239	59.434279
2332.942584	88542.594136	59.439284
2332.350758	88382.542966	59.444289
2331.435834	88209.572979	59.449293
2330.949178	88023.926706	59.454298
2330.297721	87843.627162	59.459303
2329.719421	87671.229395	59.464308
2329.022336	87498.205203	59.469313
2328.366713	87327.984243	59.474317
2328.051956	87143.757360	59.479322
2326.804149	86968.390395	59.484327
2326.491441	86776.692139	59.489332
2325.755543	86618.762565	59.494337
2324.653584	86434.298917	59.499341
2324.100047	86258.174721	59.504346
2323.500006	86090.648930	59.509351
2323.066233	85899.301017	59.514356
2322.158980	85744.821852	59.519361
2321.522826	85575.163222	59.524365
2321.356364	85388.126072	59.529370
2320.363049	85225.962470	59.534375
2319.956923	85027.740265	59.539380
2319.260535	84860.632424	59.544385
2318.061423	84682.867762	59.549389
2317.685063	84497.050740	59.554394
2316.852129	84327.515674	59.559399
2316.642590	84148.273790	59.564404
2315.554811	83978.705868	59.569409
2315.071848	83793.831009	59.574413
2314.418496	83627.176108	59.579418
2313.609060	83457.067498	59.584423
2312.977371	83281.347998	59.589428
2312.582254	83098.987955	59.594433
2311.760026	82917.039489	59.599437
2311.395327	82741.713153	59.604442
2310.450388	82578.243853	59.609447
2309.914019	82383.724204	59.614452
2309.210924	82216.879208	59.619457
2308.362176	82034.536967	59.624461
2308.051994	81860.356525	59.629466
2307.195414	81685.522653	59.634471
2306.763496	81498.974023	59.639476
2306.107997	81324.402827	59.644481
2305.405849	81136.791184	59.649485
2304.957215	80951.840859	59.654490
2303.827300	80778.807127	59.659495
2303.640541	80589.470914	59.664500
2302.401037	80426.299673	59.669505
2301.685268	80243.742880	59.674509
2301.352367	80063.408426	59.679514
2300.864054	79884.247240	59.684519
2299.963634	79709.069382	59.689524
2299.532424	79542.741377	59.694529
2298.402689	79356.398706	59.699533
2297.880754	79164.473412	59.704538
2297.295929	78996.615247	59.709543
2296.490642	78817.291793	59.714548
2296.166778	78649.534486	59.719553
2295.249984	78474.857658	59.724557
2294.894908	78278.801530	59.729562
2293.780250	78121.540977	59.734567
2293.301923	77928.555726	59.739572
2292.966456	77745.282727	59.744577
2292.372436	77573.280817	59.749581
2291.757415	77389.370988	59.754586
2290.560532	77221.795502	59.759591
2290.205961	77027.500148	59.764596
2289.298527	76844.965914	59.769601
2288.578101	76672.725514	59.774605
2288.000319	76491.776937	59.779610
2287.377941	76317.179582	59.784615
2286.604249	76125.081941	59.789620
2286.214754	75944.368160	59.794625
2285.611629	75776.849813	59.799629
2285.016457	75594.163250	59.804634
2283.976266	75416.681011	59.809639
2283.595619	75236.320621	59.814644
2282.605358	75063.794548	59.819649
2281.942668	74887.853713	59.824653
2281.775258	74698.644935	59.829658
2280.796731	74532.729682	59.834663
2279.984582	74353.370626	59.839668
2279.396136	74161.167248	59.844673
2278.789135	73980.841324	59.849677
2278.013807	73805.060867	59.854682
2277.294228	73642.273276	59.859687
2276.762136	73453.412813	59.864692
2276.085528	73278.001443	59.869697
2275.443073	73086.456795	59.874701
2274.789866	72917.456090	59.879706
2274.063902	72738.763011	59.884711
2273.709000	72563.807362	59.889716
2273.124767	72385.266019	59.894721
2271.964189	72192.342419	59.899725
2271.546379	72010.895658	59.904730
2270.919088	71855.760504	59.909735
2270.514762	71666.383584	59.914740
2269.495983	71490.396081	59.919745
2268.683903	71309.189303	59.924750
2268.136700	71133.301216	59.929754
2267.695184	70959.063908	59.934759
2266.861190	70780.475267	59.939764
2266.109183	70597.599520	59.944769
2265.456308	70412.568740	59.949774
2265.206863	70239.656531	59.954778
2264.245832	70059.320971	59.959783
2263.917700	69868.847035	59.964788
2263.475315	69690.959924	59.969793
2261.997157	69516.538740	59.974798
2261.641218	69320.114196	59.979802
2260.993723	69136.969427	59.984807
2260.771029	68963.519486	59.989812
2260.007720	68790.340506	59.994817
2259.093904	68603.493352	59.999822
2258.496927	68406.913519	60.004826
2257.766719	68240.441543	60.009831
2257.315565	68050.277149	60.014836
2256.637086	67866.648850	60.019841
2255.874473	67683.092630	60.024846
2255.504396	67501.255566	60.029850
2254.327723	67311.764468	60.034855
2253.790492	67123.383455	60.039860
2253.037043	66955.950838	60.044865
2252.466066	66768.120119	60.049870
2251.893056	66593.993200	60.054874
2251.122170	66416.153239	60.059879
2250.670247	66214.085012	60.064884
2249.943824	66041.960121	60.069889
2249.087582	65862.314919	60.074894
2248.654215	65680.859634	60.079898
2247.878287	65502.576100	60.084903
2247.637340	65306.249886	60.089908
2246.426555	65134.846363	60.094913
2245.677586	64948.214138	60.099918
2245.403267	64769.987659	60.104922
2244.585637	64584.978314	60.109927
2243.959453	64404.053270	60.114932
2243.363563	64212.208217	60.119937
2242.771788	64027.871321	60.124942
2242.192256	63853.092711	60.129946
2241.141670	63668.866882	60.134951
2240.649334	63473.147060	60.139956
2239.756231	63310.121666	60.144961
2238.885963	63128.744031	60.149966
2238.442399	62934.082618	60.154970
2237.302532	62764.661511	60.159975
2236.890266	62582.538938	60.164980
2236.350716	62407.181578	60.169985
2235.316062	62226.376836	60.174990
2234.909861	62054.436512	60.179994
2234.190043	61884.332989	60.184999
2233.907836	61700.004393	60.190004
2232.833119	61529.355703	60.195009
2232.455500	61349.094610	60.200014
2232.114776	61166.638757	60.205018
2231.254075	60993.339815	60.210023
2230.517500	60808.075841	60.215028
2229.942534	60635.225541	60.220033
2229.353202	60449.178848	60.225038
2228.727635	60259.967918	60.230042
2227.982166	60087.580212	60.235047
2227.220252	59898.907358	60.240052
2226.534444	59730.429121	60.245057
2225.634344	59546.333597	60.250062
2225.628177	59364.038448	60.255066
2224.478079	59185.341902	60.260071
2223.802907	59013.263151	60.265076
2223.658071	58821.907754	60.270081
2222.767492	58642.156039	60.275086
2222.227734	58455.364833	60.280090
2221.456407	58267.279702	60.285095
2220.761273	58093.633203	60.290100
2220.539366	57904.799914	60.295105
2219.225829	57725.310902	60.300110
2219.202765	57532.414403	60.305114
2218.742375	57364.010448	60.310119
2217.762335	57173.763507	60.315124
2216.825420	56983.749056	60.320129
2215.963109	56806.207128	60.325134
2215.508738	56617.468155	60.330138
2214.443179	56442.579322	60.335143
2214.339893	56247.616993	60.340148
2213.641674	56067.476830	60.345153
2212.607730	55892.167298	60.350158
2212.542507	55698.850416	60.355162
2211.772745	55519.116238	60.360167
2211.123210	55323.304117	60.365172
2210.314584	55143.782322	60.370177
2209.977725	54956.222172	60.375182
2209.063783	54762.094089	60.380186
2208.271610	54583.888470	60.385191
2207.784305	54389.541608	60.390196
2206.865305	54204.353626	60.395201
2206.068152	54030.597106	60.400206
2205.689697	53841.156349	60.405210
2204.858425	53664.168395	60.410215
2204.401015	53479.490479	60.415220
2203.576258	53292.648207	60.420225
2202.801612	53108.549660	60.425230
2202.170832	52924.363712	60.430234
2201.504481	52757.243525	60.435239
2201.092315	52563.970596	60.440244
2200.308294	52387.237578	60.445249
2199.470272	52199.940388	60.450254
2199.039162	52009.163386	60.455258
2198.459158	51840.471757	60.460263
2197.523747	51653.426664	60.465268
2197.004082	51460.745789	60.470273
2196.441164	51274.923787	60.475278
2195.619309	51096.886888	60.480282
2195.126576	50909.611617	60.485287
2194.508490	50724.367231	60.490292
2193.638491	50544.388187	60.495297
2192.972797	50357.003750	60.500302
2192.131331	50174.388462	60.505306
2191.363659	50001.700592	60.510311
2190.707813	49810.653556	60.515316
2190.063260	49638.082543	60.520321
2189.416379	49459.682997	60.525326
2189.481105	49268.037095	60.530330
2188.779545	49086.347165	60.535335
2187.978822	48900.726732	60.540340
2187.665016	48721.437078	60.545345
2186.401451	48530.490680	60.550350
2186.133611	48334.621088	60.555354
2185.347286	48140.949056	60.560359
2184.395900	47968.294236	60.565364
2184.053029	47781.252629	60.570369
2183.250592	47594.538967	60.575374
2182.929096	47410.072816	60.580378
2181.734985	47228.201689	60.585383
2181.161236	47038.322862	60.590388
2180.356981	46857.516645	60.595393
2179.756148	46668.737387	60.600398
2179.169000	46493.559307	60.605402
2178.746598	46299.716880	60.610407
2178.216786	46106.333289	60.615412
2177.691913	45921.076782	60.620417
2176.498322	45735.384286	60.625422
2176.077648	45542.685442	60.630426
2175.163825	45355.684252	60.635431
2174.703467	45170.694285	60.640436
2173.824190	44986.291435	60.645441
2172.887788	44801.697175	60.650446
2172.529787	44620.169545	60.655450
2172.047314	44430.633379	60.660455
2171.198658	44254.794907	60.665460
2170.679398	44065.458309	60.670465
2169.851840	43881.384691	60.675470
2169.234361	43697.950164	60.680474
2168.362951	43515.427562	60.685479
2167.768397	43326.604314	60.690484
2167.386559	43148.147654	60.695489
2166.686489	42963.801051	60.700494
2166.291217	42776.372124	60.705498
2165.351400	42593.930164	60.710503
2164.568551	42393.980544	60.715508
2164.036001	42218.593239	60.720513
2163.260603	42037.949402	60.725518
2162.761594	41841.085499	60.730522
2162.243112	41669.360276	60.735527
2161.266797	41475.495007	60.740532
2160.641238	41285.035672	60.745537
2159.773349	41108.517573	60.750542
2159.462072	40923.052810	60.755546
2158.327397	40743.874039	60.760551
2157.829833	40557.339225	60.765556
2157.248916	40362.927351	60.770561
2156.625889	40185.518263	60.775566
2156.151194	39992.431249	60.780570
2155.036526	39833.539372	60.785575
2154.591774	39643.147061	60.790580
2154.164222	39463.516969	60.795585
2153.505171	39279.562233	60.800590
2152.633905	39093.896284	60.805594
2151.856936	38907.023852	60.810599
2151.326992	38727.166410	60.815604
2150.681404	38545.305763	60.820609
2149.651232	38367.676666	60.825614
2149.297181	38182.175738	60.830618
2148.475871	37997.000731	60.835623
2147.807280	37830.051770	60.840628
2147.239749	37644.151147	60.845633
2146.359135	37460.244946	60.850638
2146.264411	37276.843600	60.855642
2145.858537	37091.881307	60.860647
2144.869872	36911.338218	60.865652
2144.227940	36727.119192	60.870657
2143.576522	36540.431569	60.875662
2143.112517	36343.725191	60.880666
2142.231698	36160.806851	60.885671
2141.398351	35977.106905	60.890676
2140.906631	35791.208356	60.895681
2140.003392	35602.976303	60.900686
2139.620564	35414.336626	60.905690
2138.754090	35247.789203	60.910695
2137.963278	35052.719251	60.915700
2137.265829	34869.071523	60.920705
2136.385934	34697.929350	60.925710
2136.252753	34509.178080	60.930714
2135.551160	34331.202819	60.935719
2134.760379	34144.235264	60.940724
2134.384371	33967.756285	60.945729
2133.621472	33785.352511	60.950734
2133.066845	33600.613528	60.955738
2132.163819	33412.159600	60.960743
2131.851880	33208.504563	60.965748
2131.123886	33038.755506	60.970753
2130.294085	32856.677541	60.975758
2129.893494	32665.064496	60.980762
2129.181743	32482.580004	60.985767
2128.306206	32293.080405	60.990772
2127.781591	32099.101114	60.995777
2126.954061	31921.108460	61.000782
2126.519168	31734.697848	61.005786
2125.459661	31545.087484	61.010791
2125.106878	31364.672646	61.015796
2124.200365	31159.143030	61.020801
2123.300129	30992.779548	61.025806
2122.968382	30804.212568	61.030810
2122.166947	30628.539837	61.035815
2121.481321	30435.874476	61.040820
2121.166767	30262.443195	61.045825
2120.416444	30070.489187	61.050830
2119.894488	29878.784015	61.055834
2118.949094	29703.535880	61.060839
2118.092874	29514.841003	61.065844
2117.768986	29338.727141	61.070849
2116.665402	29154.891361	61.075854
2116.386025	28964.995878	61.080858
2115.513189	28792.150643	61.085863
2115.032995	28608.327967	61.090868
2114.249446	28420.620063	61.095873
2113.375481	28239.529259	61.100878
2113.344361	28047.808795	61.105882
2112.386354	27866.180968	61.110887
2111.564219	27688.930173	61.115892
2111.551901	27500.540224	61.120897
2110.352514	27324.091030	61.125902
2109.954708	27126.518710	61.130906
2109.060859	26951.280992	61.135911
2108.555166	26763.098754	61.140916
2107.880910	26582.664570	61.145921
2107.033588	26394.348114	61.150926
2106.378256	26205.841479	61.155930
2105.553535	26029.459137	61.160935
2105.220750	25853.171268	61.165940
2104.642271	25657.402914	61.170945
2103.381162	25479.768984	61.175950
2103.348132	25287.219109	61.180954
2102.550627	25112.056400	61.185959
2101.643169	24921.974735	61.190964
2100.978290	24752.976356	61.195969
2100.601602	24560.270971	61.200974
2100.031124	24376.124609	61.205978
2099.407236	24187.451088	61.210983
2098.682029	23998.850362	61.215988
2097.684250	23814.055689	61.220993
2097.034166	23637.649050	61.225998
2096.702122	23453.424950	61.231002
2096.059638	23265.512321	61.236007
2095.103860	23082.611534	61.241012
2094.405923	22890.162064	61.246017
2093.850975	22715.598346	61.251022
2093.303218	22523.904917	61.256026
2092.204548	22351.087361	61.261031
2091.582191	22165.780064	61.266036
2091.183894	21977.806015	61.271041
2090.077899	21816.119544	61.276046
2089.831888	21628.820326	61.281050
2088.968236	21443.011795	61.286055
2088.041366	21267.549483	61.291060
2087.683969	21088.108546	61.296065
2086.954882	20911.123366	61.301070
2086.395618	20731.933272	61.306074
2085.212302	20552.751865	61.311079
2084.686318	20381.780012	61.316084
2084.194709	20198.019775	61.321089
2083.457247	20029.394670	61.326094
2082.747076	19854.354266	61.331098
2082.007425	19682.201373	61.336103
2081.287125	19506.928811	61.341108
2080.631673	19342.553820	61.346113
2080.041558	19170.869923	61.351118
2079.786343	18986.959642	61.356122
2078.695902	18818.092923	61.361127
2078.167992	18652.583912	61.366132
2077.770094	18467.835562	61.371137
2076.951171	18299.844740	61.376142
2076.174746	18126.717747	61.381146
2075.556204	17954.488472	61.386151
2074.909626	17777.345593	61.391156
2074.467895	17603.528333	61.396161
2073.462910	17433.106763	61.401166
2072.805867	17255.626128	61.406170
2071.982978	17083.097914	61.411175
2071.368934	16911.575498	61.416180
2070.822794	16732.587210	61.421185
2069.974827	16567.521162	61.426190
2069.355416	16403.524290	61.431194
2068.675787	16235.359038	61.436199
2068.107953	16071.802279	61.441204
2067.415251	15884.792668	61.446209
2066.252021	15731.607812	61.451214
2066.088598	15557.099804	61.456218
2065.077761	15402.521161	61.461223
2064.469592	15236.499725	61.466228
2063.880365	15067.975890	61.471233
2062.939175	14920.145370	61.476238
2062.339835	14743.884665	61.481242
2061.768219	14592.345216	61.486247
2060.959129	14427.099080	61.491252
2060.244852	14266.613690	61.496257
2059.291919	14112.926327	61.501262
2059.082624	13948.708180	61.506266
2057.938141	13794.683550	61.511271
2057.155172	13639.162334	61.516276
2056.703706	13487.697692	61.521281
2055.741638	13342.907938	61.526286
2055.258512	13185.174701	61.531290
2054.387898	13042.757872	61.536295
2053.813853	12890.598981	61.541300
2052.764085	12751.523701	61.546305
2051.720289	12612.766764	61.551310
2051.177681	12468.490494	61.556314
2050.443420	12332.769924	61.561319
2049.204926	12207.211956	61.566324
2048.592187	12068.204751	61.571329
2047.413520	11950.540775	61.576334
2046.689847	11844.954072	61.581338
2045.649602	11728.954375	61.586343
2045.040867	11616.330857	61.591348
2044.409548	11514.861481	61.596353
2043.037481	11410.966555	61.601358
2042.516941	11302.525707	61.606362
2041.774661	11214.575379	61.611367
2040.754360	11130.769255	61.616372
2039.729394	11054.042578	61.621377
2038.301622	10972.902732	61.626382
2037.603371	10886.860384	61.631386
2036.784254	10829.337239	61.636391
2036.011465	10753.374134	61.641396
2035.694275	10686.632007	61.646401
2034.336055	10627.359491	61.651406
2034.322210	10566.102078	61.656410
2033.540785	10499.505861	61.661415
2032.809773	10434.463616	61.666420
2032.517281	10374.577949	61.671425
2031.747982	10323.915294	61.676430
2031.307492	10244.509623	61.681434
2030.129913	10180.929393	61.686439
2029.321438	10126.056351	61.691444
2029.151447	10052.640344	61.696449
2027.962506	10011.292885	61.701454
2027.548177	9943.390295	61.706458
2027.052264	9892.497528	61.711463
2026.430978	9838.933176	61.716468
2025.861225	9770.881268	61.721473
2025.149609	9724.520946	61.726478
2024.700182	9664.302439	61.731482
2023.874877	9600.695582	61.736487
2023.063976	9540.829228	61.741492
2022.760339	9482.903962	61.746497
2021.753820	9442.655778	61.751502
2021.395204	9367.671824	61.756506
2020.942020	9310.050648	61.761511
2020.360627	9256.555414	61.766516
2019.977722	9182.222795	61.771521
2019.022452	9122.331319	61.776526
2018.449900	9064.805374	61.781530
2017.769192	9010.324809	61.786535
2016.945328	8940.860981	61.791540
2016.609823	8876.388143	61.796545
2015.295675	8821.081397	61.801550
2014.968857	8758.413574	61.806554
2014.416452	8699.687042	61.811559
2013.991382	8636.908695	61.816564
2013.601642	8572.342027	61.821569
2012.516851	8516.772795	61.826574
2012.222377	8449.993589	61.831578
2011.370628	8382.939041	61.836583
2010.496539	8332.290277	61.841588
2010.413996	8261.064295	61.846593
2009.280828	8208.398405	61.851598
2008.552784	8127.852389	61.856602
2008.020584	8074.708576	61.861607
2007.292668	8002.705051	61.866612
2006.407201	7954.999990	61.871617
2005.762289	7907.465959	61.876622
2005.395844	7831.328496	61.881626
2004.616721	7776.473206	61.886631
2004.085857	7720.707000	61.891636
2003.520329	7664.484221	61.896641
2002.412584	7588.972111	61.901646
2001.778896	7544.407575	61.906650
2001.413369	7476.247293	61.911655
2000.488675	7420.723001	61.916660
2000.035036	7364.530925	61.921665
1999.368185	7307.279540	61.926670
1998.928612	7252.219249	61.931674
1998.248135	7193.183701	61.936679
1997.103266	7136.592991	61.941684
1996.821772	7065.163290	61.946689
1996.327508	7021.927909	61.951694
1995.701967	6956.340315	61.956698
1994.750917	6895.312102	61.961703
1994.197040	6839.573356	61.966708
1993.563118	6767.379842	61.971713
1992.928217	6709.762034	61.976718
1992.143259	6654.513447	61.981722
1991.552826	6587.492553	61.986727
1990.798099	6541.297650	61.991732
1990.593309	6468.350413	61.996737
1989.637553	6423.236123	62.001742
1988.775287	6362.995865	62.006746
1988.284902	6302.714180	62.011751
1987.468483	6249.056813	62.016756
1986.746123	6191.874541	62.021761
1986.060683	6141.081426	62.026766
1985.668478	6079.761202	62.031770
1984.995404	6020.212479	62.036775
1984.135005	5962.799798	62.041780
1983.788761	5904.144637	62.046785
1982.916861	5851.705149	62.051790
1982.524022	5783.883513	62.056794
1981.903585	5731.854141	62.061799
1981.098919	5663.567575	62.066804
1980.494514	5603.462220	62.071809
1979.771504	5546.702168	62.076814
1979.123982	5491.485008	62.081818
1978.325078	5423.841478	62.086823
1977.566081	5384.856989	62.091828
1977.281600	5317.402838	62.096833
1976.580416	5261.874819	62.101838
1975.923885	5205.998392	62.106842
1975.230103	5135.528391	62.111847
1974.637993	5085.501791	62.116852
1974.122682	5012.594437	62.121857
1973.011402	4962.138770	62.126862
1972.376930	4904.027071	62.131866
1972.020501	4842.782798	62.136871
1970.995194	4799.186254	62.141876
1970.401414	4724.925122	62.146881
1969.665679	4683.791099	62.151886
1969.321313	4603.658389	62.156890
1968.561222	4557.064351	62.161895
1967.676236	4504.044926	62.166900
1967.408229	4433.475992	62.171905
1966.229942	4390.539853	62.176910
1965.843763	4335.764280	62.181914
1965.256893	4284.719772	62.186919
1964.407459	4224.602138	62.191924
1963.942973	4161.365880	62.196929
1963.301315	4113.587969	62.201934
1962.508475	4052.484079	62.206938
1962.003768	3992.249581	62.211943
1961.288695	3949.792496	62.216948
1960.684539	3880.106898	62.221953
1959.599109	3833.651973	62.226958
1959.141332	3762.145517	62.231962
1958.687611	3703.813484	62.236967
1957.782516	3651.457290	62.241972
1957.211622	3598.070290	62.246977
1956.408823	3549.621825	62.251982
1955.907003	3482.557574	62.256986
1955.260280	3436.284276	62.261991
1954.350948	3385.397393	62.266996
1954.247237	3330.128040	62.272001
1953.292599	3266.274693	62.277006
1952.434783	3220.224072	62.282010
1952.041460	3162.629870	62.287015
1950.912400	3120.706201	62.292020
1950.672800	3058.871156	62.297025
1949.745618	2997.694405	62.302030
1949.250961	2945.986927	62.307034
1948.688413	2897.459109	62.312039
1947.835299	2843.706415	62.317044
1947.905088	2772.294532	62.322049
1946.559973	2729.437069	62.327054
1946.131386	2671.721850	62.332058
1945.580631	2607.215018	62.337063
1944.715374	2556.939926	62.342068
1944.146983	2506.703840	62.347073
1943.424878	2460.097032	62.352078
1942.694354	2390.116036	62.357082
1941.949215	2351.631859	62.362087
1940.986821	2298.422148	62.367092
1940.859908	2235.340119	62.372097
1940.093220	2194.009813	62.377102
1939.769503	2132.563456	62.382106
1938.973246	2082.465152	62.387111
1937.925469	2028.450643	62.392116
1937.417109	1977.638283	62.397121
1936.619924	1910.279570	62.402126
1936.239523	1860.595467	62.407130
1935.634306	1809.520702	62.412135
1934.628039	1751.213979	62.417140
1934.079985	1697.643399	62.422145
1933.445381	1645.008581	62.427150
1932.779679	1604.610976	62.432154
1932.368388	1546.926631	62.437159
1931.398959	1493.893670	62.442164
1930.677018	1437.178524	62.447169
1929.720733	1387.921796	62.452174
1928.898430	1334.395300	62.457178
1928.193769	1286.406375	62.462183
1927.470929	1246.654399	62.467188
1927.356672	1193.077529	62.472193
1926.378435	1164.035198	62.477198
1926.253516	1101.073667	62.482202
1925.532133	1055.393819	62.487207
1924.564315	1003.110707	62.492212
1923.917454	958.529577	62.497217
1923.219737	919.369054	62.502222
1922.684572	855.688345	62.507226
1922.000941	816.376046	62.512231
1921.369772	767.973448	62.517236
1920.774549	712.451380	62.522241
1919.854159	678.062642	62.527246
1919.144367	619.856116	62.532250
1918.807405	585.415981	62.537255
1918.078092	526.272247	62.542260
1917.337734	491.346002	62.547265
1916.402099	449.568864	62.552270
1915.992841	391.377048	62.557274
1915.020776	353.111603	62.562279
1914.050894	308.432362	62.567284
1913.409270	264.093814	62.572289
1912.797149	231.740375	62.577294
1912.069840	196.396454	62.582298
1911.949727	151.095516	62.587303
1910.837885	107.894963	62.592308
1909.893136	77.504364	62.597313
1909.293443	40.670849	62.602318
1908.335108	4.097789	62.607322
1907.564347	-24.544581	62.612327
1906.748572	-44.148645	62.617332
1906.011700	-66.198415	62.622337
1902.185084	-0.931614	62.627342
1900.725072	13.278372	62.632346
1901.096621	20.904023	62.637351
1901.279140	22.207765	62.642356
1901.831644	15.385137	62.647361
1901.742769	18.687371	62.652366
1900.958150	16.079298	62.657370
1899.196247	18.729358	62.662375
1898.200089	19.017018	62.667380
1897.799336	30.863754	62.672385
1896.713235	29.800061	62.677390
1896.569888	29.070820	62.682394
1896.263400	32.625223	62.687399
1895.311077	30.676128	62.692404
1895.530110	25.846075	62.697409
1894.538240	38.360670	62.702414
1893.945544	30.265903	62.707418
1893.235339	30.815671	62.712423
1892.389954	39.385155	62.717428
1892.014150	28.401689	62.722433
1890.874451	37.617136	62.727438
1889.869181	29.378138	62.732442
1889.391454	41.426337	62.737447
1888.249213	44.559923	62.742452
1888.892212	31.333142	62.747457
1888.282954	36.534635	62.752462
1887.801279	42.116419	62.757466
1887.092697	36.517428	62.762471
1885.521392	28.396684	62.767476
1884.937500	40.026500	62.772481
1884.128298	38.687040	62.777486
1883.698636	32.740996	62.782490
1883.344666	31.680921	62.787495
1882.173949	37.555024	62.792500
1881.971760	25.738181	62.797505
1881.069036	41.575438	62.802510
1880.998839	36.524797	62.807514
1880.058420	29.773604	62.812519
1879.244898	42.494855	62.817524
1879.357246	29.885330	62.822529
1877.723437	43.738174	62.827534
1877.497113	45.458485	62.832538
1877.088657	30.454268	62.837543
1875.691474	40.152146	62.842548
1875.482029	32.493273	62.847553
1875.245088	38.474592	62.852558
1874.238552	41.663907	62.857562
1873.247099	35.087973	62.862567
1872.379327	39.770699	62.867572
1872.323382	33.683322	62.872577
1872.048742	44.485035	62.877582
1870.800345	30.579265	62.882586
1869.978761	31.309147	62.887591
1869.543600	51.195887	62.892596
1869.258148	27.948383	62.897601
1867.972968	45.527389	62.902606
1867.302928	26.516696	62.907610
1867.417545	48.440284	62.912615
1866.353712	40.144358	62.917620
1865.343426	36.034603	62.922625
1864.472725	37.133405	62.927630
1864.243178	38.165104	62.932634
1864.074494	31.665123	62.937639
1863.011408	37.840687	62.942644
1862.211664	29.211105	62.947649
1861.302195	43.002567	62.952654
1861.355260	27.420460	62.957658
1860.417809	33.804732	62.962663
1859.268222	41.572553	62.967668
1859.418771	37.064026	62.972673
1858.062735	33.868604	62.977678
1857.410738	31.176408	62.982682
1857.304111	27.172338	62.987687
1856.583098	46.245023	62.992692
1856.061343	29.282892	62.997697
1855.125316	42.279062	63.002702
1854.645156	32.037566	63.007706
1854.228334	42.262614	63.012711
1853.622545	35.584454	63.017716
1853.087730	31.578984	63.022721
1851.527550	23.984774	63.027726
1850.438638	43.907494	63.032730
1850.821591	33.429609	63.037735
1849.897794	43.512804	63.042740
1849.058883	27.097773	63.047745
1848.323391	45.133551	63.052750
1847.826814	41.746478	63.057754
1846.929605	27.139996	63.062759
1846.810426	41.542411	63.067764
1846.255096	35.662060	63.072769
1845.276207	34.628674	63.077774
1844.530894	35.822690	63.082778
1843.883865	28.812042	63.087783
1843.477009	41.416689	63.092788
1843.216013	32.873458	63.097793
1842.342000	41.064303	63.102798
1841.250603	38.708381	63.107802
1840.315902	35.523339	63.112807
1839.419473	38.483873	63.117812
1839.726888	42.804972	63.122817
1838.701350	40.302976	63.127822
1837.564854	40.330669	63.132826
1837.255320	25.036376	63.137831
1836.426736	48.495849	63.142836
1836.020411	32.313328	63.147841
1835.461072	45.645506	63.152846
1834.937269	36.264069	63.157850
1834.370386	36.130357	63.162855
1833.804583	31.874347	63.167860
1833.538842	34.905049	63.172865
1832.302553	36.788881	63.177870
1831.079824	40.553430	63.182874
1830.523282	34.736354	63.187879
1829.632956	38.503316	63.192884
1829.403883	23.339752	63.197889
1828.460004	36.669904	63.202894
1828.056470	31.235385	63.207898
1827.786824	39.576272	63.212903
1826.637525	33.612046	63.217908
1826.496483	40.702498	63.222913
1825.963879	23.543414	63.227918
1825.349206	33.621679	63.232922
1823.973203	28.805197	63.237927
1822.945018	32.978824	63.242932
1823.050722	30.997372	63.247937
1821.982699	35.781294	63.252942
1821.220988	38.351438	63.257946
1821.103330	23.715806	63.262951
1820.338319	38.763233	63.267956
1820.160215	24.206585	63.272961
1819.493922	30.369617	63.277966
1818.512295	33.143413	63.282970
1817.752809	29.258782	63.287975
1816.474964	27.711488	63.292980
1815.872827	31.929427	63.297985
1815.327268	30.726321	63.302990
1814.785965	38.015946	63.307994
1814.384447	22.116530	63.312999
1813.971487	25.422919	63.318004
1813.498215	23.011437	63.323009
1812.958494	27.913319	63.328014
1811.994395	33.453442	63.333018
1811.130421	28.591933	63.338023
1809.987752	33.952256	63.343028
1809.598007	28.245896	63.348033
1808.884402	37.701214	63.353038
1808.409985	26.466927	63.358042
1808.448237	36.417862	63.363047
1807.500008	29.163320	63.368052
1806.287109	26.449820	63.373057
1805.634350	35.234737	63.378062
1804.953026	37.509847	63.383066
1804.452647	28.911598	63.388071
1803.820687	36.693433	63.393076
1803.738135	23.660711	63.398081
1802.885593	38.277342	63.403086
1801.508189	32.803510	63.408090
1800.671246	23.804551	63.413095
1799.979049	30.766478	63.418100
1799.387733	31.765743	63.423105
1799.442425	27.384404	63.428110
1798.868441	31.378681	63.433114
1798.303333	35.620706	63.438119
1797.347088	33.768465	63.443124
1797.319997	25.711648	63.448129
1796.037749	23.646250	63.453134
1795.031299	28.802021	63.458138
1794.849338	36.323165	63.463143
1794.274629	37.710876	63.468148
1793.395628	29.019791	63.473153
1792.755394	36.342475	63.478158
1791.638437	34.086828	63.483162
1791.379740	37.144800	63.488167
1790.581672	30.326886	63.493172
1790.566869	27.924605	63.498177
1789.335013	26.772141	63.503182
1788.166547	32.276916	63.508186
1787.754751	32.068124	63.513191
1786.971401	30.986363	63.518196
1786.282035	26.291099	63.523201
1785.829446	33.755871	63.528206
1785.270920	26.858921	63.533210
1784.871977	30.838019	63.538215
1784.221083	36.944999	63.543220
1783.867827	26.468911	63.548225
1783.364931	44.825723	63.553230
1781.994205	39.478572	63.558234
1781.916736	22.501118	63.563239
1781.094843	32.571293	63.568244
1780.060572	30.878105	63.573249
1778.815133	30.532043	63.578254
1778.037512	34.535009	63.583258
1778.098504	29.930320	63.588263
1777.301753	27.455098	63.593268
1777.211889	36.106475	63.598273
1776.699648	31.941322	63.603278
1775.594367	35.211006	63.608282
1774.710491	27.862681	63.613287
1773.447460	40.551255	63.618292
1773.085910	35.840203	63.623297
1772.543875	24.569359	63.628302
1772.103092	33.501964	63.633306
1771.767236	18.489419	63.638311
1771.540914	36.020136	63.643316
1771.107172	25.577334	63.648321
1769.799691	31.615121	63.653326
1768.374361	23.953822	63.658330
1768.089451	19.501839	63.663335
1767.455011	40.618679	63.668340
1767.235127	32.226628	63.673345
1766.628502	40.450721	63.678350
1765.365758	35.390783	63.683354
1764.761719	27.264744	63.688359
1764.173441	33.218281	63.693364
1763.932242	24.774427	63.698369
1763.345430	24.156621	63.703374
1762.068215	27.377920	63.708378
1761.491977	26.928744	63.713383
1760.704652	34.579141	63.718388
1760.314983	23.988997	63.723393
1759.889984	38.307503	63.728398
1759.305105	25.453910	63.733402
1758.655078	29.802466	63.738407
1757.167487	28.916134	63.743412
1756.865148	29.129930	63.748417
1756.661617	40.161617	63.753422
1755.693310	32.124968	63.758426
1755.701305	27.541313	63.763431
1754.303947	31.846131	63.768436
1754.135368	24.146101	63.773441
1753.602356	24.204144	63.778446
1752.844408	20.385525	63.783450
1751.906119	27.880124	63.788455
1751.032356	42.143749	63.793460
1750.457909	25.983234	63.798465
1750.105040	25.629472	63.803470
1748.772116	22.603906	63.808474
1748.024782	22.653412	63.813479
1746.890325	33.139084	63.818484
1746.599739	34.241987	63.823489
1746.515756	25.301662	63.828494
1745.644278	25.575886	63.833498
1744.607510	31.171725	63.838503
1744.115629	27.444890	63.843508
1743.863162	30.527105	63.848513
1743.284118	26.353648	63.853518
1742.646489	38.159166	63.858522
1742.636474	19.802227	63.863527
1741.198108	22.356852	63.868532
1740.649188	28.548565	63.873537
1740.053591	25.213516	63.878542
1739.505997	29.403883	63.883546
1738.719542	22.235645	63.888551
1737.442646	28.421550	63.893556
1737.108668	23.756592	63.898561
1736.789881	26.559183	63.903566
1735.918311	23.332620	63.908570
1735.569976	24.250731	63.913575
1734.422885	33.500517	63.918580
1733.935704	24.573769	63.923585
1733.260188	26.039002	63.928590
1732.656107	36.227560	63.933594
1732.390697	26.601697	63.938599
1730.918046	36.470891	63.943604
1730.431262	30.070335	63.948609
1729.557592	30.084718	63.953614
1729.041748	24.177632	63.958618
1728.772977	30.230238	63.963623
1728.226809	27.972275	63.968628
1727.827360	33.582016	63.973633
1727.238846	28.306208	63.978638
1726.527187	36.682604	63.983642
1725.581657	23.687610	63.988647
1724.289882	35.179134	63.993652
1723.779144	26.541555	63.998657
1723.229915	31.438653	64.003662
1722.381148	34.221343	64.008666
1722.432831	33.112633	64.013671
1721.663205	27.338895	64.018676
1720.817306	24.546649	64.023681
1720.334421	32.820476	64.028686
1719.656620	37.223916	64.033690
1718.899587	29.809736	64.038695
1717.689452	37.749646	64.043700
1716.946270	27.403314	64.048705
1716.527785	35.157564	64.053710
1715.653903	26.292238	64.058714
1715.362624	30.408784	64.063719
1714.845880	34.031289	64.068724
1714.413825	26.278495	64.073729
1714.138475	28.034986	64.078734
1712.979485	28.831122	64.083738
1712.731032	23.427193	64.088743
1711.639486	34.634608	64.093748
1710.794807	25.108640	64.098753
1710.045520	29.044044	64.103758
1709.115867	25.128132	64.108762
1708.920625	27.434867	64.113767
1708.302621	21.555053	64.118772
1708.002553	30.304464	64.123777
1706.882299	28.464115	64.128782
1705.994852	30.292597	64.133786
1705.450914	27.898668	64.138791
1704.773290	30.275714	64.143796
1704.484857	19.541776	64.148801
1703.710591	29.654863	64.153806
1702.538728	30.804706	64.158810
1702.272752	20.880901	64.163815
1701.439702	27.406328	64.168820
1701.158782	15.250379	64.173825
1700.778584	29.747840	64.178830
1699.799612	27.881900	64.183834
1699.174350	24.975770	64.188839
1698.443300	28.737971	64.193844
1697.766758	27.040036	64.198849
1696.656189	24.330838	64.203854
1695.629027	32.708465	64.208858
1695.563124	15.082656	64.213863
1694.506489	30.190603	64.218868
1694.498947	19.915095	64.223873
1694.290262	26.450160	64.228878
1693.108614	26.996016	64.233882
1692.347509	25.969099	64.238887
1691.690318	27.956552	64.243892
1691.218116	27.035132	64.248897
1690.990436	19.447002	64.253902
1689.755111	25.490707	64.258906
1688.850135	24.811492	64.263911
1688.115148	30.267953	64.268916
1688.070352	22.333808	64.273921
1687.670064	16.327959	64.278926
1686.499968	34.281382	64.283930
1685.862158	21.248572	64.288935
1685.182223	30.378439	64.293940
1684.270576	26.792410	64.298945
1683.434655	25.392606	64.303950
1682.271788	33.067978	64.308954
1682.300422	25.194708	64.313959
1681.714721	23.409810	64.318964
1681.353260	29.494486	64.323969
1681.483485	26.894132	64.328974
1679.868030	25.089876	64.333978
1679.001102	23.447420	64.338983
1678.327625	33.415196	64.343988
1678.056970	20.081221	64.348993
1678.012200	31.392029	64.353998
1676.658813	25.581724	64.359002
1675.958967	17.688556	64.364007
1675.207862	32.120356	64.369012
1674.520788	21.053934	64.374017
1673.328764	22.027220	64.379022
1672.166290	20.526328	64.384026
1672.419585	20.479989	64.389031
1671.926062	31.441035	64.394036
1671.570323	17.701114	64.399041
1671.099364	13.756513	64.404046
1670.065518	36.272457	64.409050
1669.271280	14.127724	64.414055
1668.040842	24.869934	64.419060
1667.410735	27.654175	64.424065
1666.941144	16.061208	64.429070
1666.647176	23.160170	64.434074
1666.514601	18.280310	64.439079
1665.530509	20.180925	64.444084
1664.539535	26.302520	64.449089
1664.193650	23.776218	64.454094
1663.278748	29.682305	64.459098
1663.487540	18.694354	64.464103
1661.878936	24.854134	64.469108
1661.057851	27.914716	64.474113
1660.798205	26.552688	64.479118
1660.176279	25.074745	64.484122
1659.162819	24.285041	64.489127
1658.442239	25.555602	64.494132
1657.867544	22.789684	64.499137
1657.448627	30.217578	64.504142
1656.948617	26.837404	64.509146
1656.404684	19.130785	64.514151
1655.043749	24.451720	64.519156
1654.787233	20.853098	64.524161
1654.293734	33.734853	64.529166
1653.435285	27.568399	64.534170
1652.620926	27.351037	64.539175
1651.577937	31.593306	64.544180
1651.145775	13.732379	64.549185
1650.724991	15.314860	64.554190
1650.231839	32.667176	64.559194
1650.079126	11.693139	64.564199
1649.041376	24.191415	64.569204
1648.283121	29.156422	64.574209
1647.977857	18.612827	64.579214
1646.813061	19.706377	64.584218
1646.044215	33.896577	64.589223
1645.411151	18.928127	64.594228
1644.884845	24.993259	64.599233
1644.486680	25.905104	64.604238
1643.316071	28.388862	64.609242
1642.605995	24.436519	64.614247
1641.709902	23.814256	64.619252
1641.218801	31.267811	64.624257
1640.973049	26.317621	64.629262
1640.460037	26.563320	64.634266
1639.921309	20.393393	64.639271
1638.977040	25.649722	64.644276
1638.193481	17.435555	64.649281
1637.888160	20.690173	64.654286
1636.847187	21.421862	64.659290
1636.419513	12.993469	64.664295
1635.182177	22.188234	64.669300
1634.511300	24.179451	64.674305
1634.888432	18.546847	64.679310
1633.639831	21.828312	64.684314
1632.936316	24.792954	64.689319
1632.301864	21.344260	64.694324
1631.693046	26.306030	64.699329
1631.534984	13.471423	64.704334
1630.150608	25.455496	64.709338
1629.774429	14.256130	64.714343
1628.992735	28.782678	64.719348
1628.527343	22.836066	64.724353
1627.416817	17.162252	64.729358
1626.587251	20.321959	64.734362
1626.218668	22.492234	64.739367
1625.985223	20.072655	64.744372
1625.126011	25.892635	64.749377
1624.677022	20.599425	64.754382
1623.569701	21.306967	64.759386
1623.318283	12.557267	64.764391
1622.691664	18.441218	64.769396
1622.017146	30.391375	64.774401
1621.095151	17.000045	64.779406
1620.211911	18.245995	64.784410
1619.821715	20.865976	64.789415
1619.410939	24.832779	64.794420
1618.515270	20.684426	64.799425
1617.686883	14.678794	64.804430
1617.106430	32.079670	64.809434
1616.687492	21.696064	64.814439
1615.674969	28.043446	64.819444
1614.592536	24.713233	64.824449
1614.198275	20.463148	64.829454
1613.804415	27.415559	64.834458
1613.795579	29.681648	64.839463
1612.990629	28.609681	64.844468
1612.026324	20.365890	64.849473
1611.036094	22.199692	64.854478
1610.339377	24.360598	64.859482
1610.457094	25.075375	64.864487
1609.022134	25.756128	64.869492
1608.326209	23.624487	64.874497
1607.847876	33.662195	64.879502
1607.025370	23.812632	64.884506
1607.072942	25.142519	64.889511
1605.688224	37.388437	64.894516
1604.974073	21.253334	64.899521
1604.598862	11.797915	64.904526
1604.135507	20.292568	64.909530
1603.554198	20.427701	64.914535
1602.265139	17.685404	64.919540
1601.684985	24.784105	64.924545
1601.643588	19.828265	64.929550
1600.659945	16.764637	64.934554
1600.165385	19.730781	64.939559
1599.177724	23.391848	64.944564
1598.694439	13.012168	64.949569
1598.294943	18.003764	64.954574
1597.362377	14.031592	64.959578
1596.571684	13.873566	64.964583
1596.043663	15.976135	64.969588
1595.401464	17.683687	64.974593
1594.629853	9.760953	64.979598
1593.602117	20.754831	64.984602
1593.391254	15.898455	64.989607
1592.499642	22.015323	64.994612
1591.949902	27.838184	64.999617
1591.805692	22.053441	65.004622
1590.655681	13.880168	65.009626
1590.268797	19.063724	65.014631
1589.534175	13.557288	65.019636
1588.656670	17.602975	65.024641
1587.699237	17.223863	65.029646
1586.627308	23.787270	65.034650
1586.756988	10.695649	65.039655
1586.506919	26.728865	65.044660
1585.965498	22.469050	65.049665
1584.879374	18.865052	65.054670
1583.981927	25.824934	65.059674
1583.600367	27.942084	65.064679
1583.035146	29.309407	65.069684
1582.226528	22.255135	65.074689
1581.442187	19.438967	65.079694
1580.442175	30.828993	65.084698
1580.721398	19.211696	65.089703
1579.123087	37.931768	65.094708
1578.289654	33.090725	65.099713
1578.195568	19.736608	65.104718
1577.078726	34.182378	65.109722
1577.124015	27.769866	65.114727
1576.524128	22.048061	65.119732
1575.691260	23.208753	65.124737
1574.669661	18.899078	65.129742
1574.155840	32.544148	65.134746
1573.947024	18.418216	65.139751
1573.081083	26.836492	65.144756
1572.088172	25.072165	65.149761
1571.737428	25.285789	65.154766
1571.040192	31.013819	65.159770
1570.238544	24.068829	65.164775
1569.371790	43.074798	65.169780
1568.551887	23.413132	65.174785
1568.345045	31.163726	65.179790
1567.936343	32.216027	65.184794
1567.474371	23.261668	65.189799
1566.276383	33.405836	65.194804
1565.541156	31.494915	65.199809
1565.288236	28.289966	65.204814
1564.023928	27.104922	65.209818
1563.471788	33.003864	65.214823
1562.865835	34.076468	65.219828
1562.134076	30.044016	65.224833
1561.994910	16.665528	65.229838
1561.090381	27.121032	65.234842
1560.338162	26.764518	65.239847
1559.532911	24.128295	65.244852
1559.465885	31.307900	65.249857
1558.541638	23.822582	65.254862
1557.448210	27.259198	65.259866
1556.687302	28.293347	65.264871
1556.247942	16.823343	65.269876
1556.205860	25.974881	65.274881
1555.303143	18.208606	65.279886
1554.206297	26.240956	65.284890
1553.848478	16.118894	65.289895
1553.256665	22.544525	65.294900
1552.097008	20.770431	65.299905
1551.882720	23.685744	65.304910
1550.837274	15.387069	65.309914
1550.828066	20.086424	65.314919
1550.004438	23.011824	65.319924
1548.768806	20.212180	65.324929
1548.523609	15.914771	65.329934
1547.993659	13.758354	65.334938
1547.438614	12.351815	65.339943
1546.441764	21.801710	65.344948
1545.554422	18.170876	65.349953
1544.886649	20.459661	65.354958
1544.652677	20.908620	65.359962
1544.364228	21.892932	65.364967
1543.071460	21.248579	65.369972
1542.151708	23.891214	65.374977
1542.064297	17.860912	65.379982
1541.342060	23.175030	65.384986
1540.258795	19.491751	65.389991
1539.706709	14.270137	65.394996
1539.039603	24.285800	65.400001
1538.878694	17.795674	65.405006
1538.091987	18.313537	65.410010
1537.303770	18.017943	65.415015
1536.258046	25.217439	65.420020
1535.782781	17.928871	65.425025
1536.088408	25.191183	65.430030
1534.666932	21.506454	65.435034
1533.915234	21.818485	65.440039
1533.635531	16.417975	65.445044
1532.528937	28.916186	65.450049
1531.760138	11.052028	65.455054
1530.925888	24.650238	65.460058
1530.713221	9.627660	65.465063
1529.992759	24.764223	65.470068
1529.410850	20.064584	65.475073
1528.655423	26.069947	65.480078
1527.860639	27.109486	65.485082
1527.474196	13.249912	65.490087
1526.976993	21.852452	65.495092
1526.006002	22.158331	65.500097
1525.623694	24.404915	65.505102
1525.038105	22.202150	65.510106
1524.109507	12.337950	65.515111
1523.194991	17.796162	65.520116
1522.258826	22.521388	65.525121
1522.184375	19.857362	65.530126
1521.468979	28.005728	65.535130
1520.471853	26.349324	65.540135
1519.562833	16.062547	65.545140
1519.163201	26.570293	65.550145
1518.977548	17.852737	65.555150
1518.186860	31.404610	65.560154
1517.707169	17.872086	65.565159
1516.474186	22.051551	65.570164
1515.912185	25.162466	65.575169
1515.770680	14.780539	65.580174
1515.205389	24.124022	65.585178
1514.312232	21.531746	65.590183
1513.571424	23.523065	65.595188
1512.721547	29.904559	65.600193
1512.062001	26.797350	65.605198
1510.742296	31.394296	65.610202
1510.294629	15.343052	65.615207
1510.005460	34.295082	65.620212
1509.633236	20.086321	65.625217
1509.613923	12.771041	65.630222
1508.585338	20.401477	65.635226
1507.739662	21.706149	65.640231
1507.141356	15.283957	65.645236
1506.075505	21.642999	65.650241
1505.480399	19.700369	65.655246
1504.820447	31.544150	65.660250
1504.465441	14.249751	65.665255
1503.539144	22.225053	65.670260
1502.681093	31.146714	65.675265
1501.959245	26.861975	65.680270
1501.645076	25.959633	65.685274
1501.392332	27.013969	65.690279
1500.236226	21.132996	65.695284
1499.440803	23.386885	65.700289
1499.238005	19.571594	65.705294
1498.275468	32.203042	65.710298
1497.436108	15.337270	65.715303
1496.761962	25.765639	65.720308
1495.853812	16.880630	65.725313
1496.085120	17.373925	65.730318
1495.304780	21.650201	65.735322
1494.664306	20.823368	65.740327
1493.802498	35.520367	65.745332
1492.841961	18.472003	65.750337
1491.995604	21.574493	65.755342
1491.105578	18.811420	65.760346
1490.690501	21.170447	65.765351
1490.315698	17.160144	65.770356
1489.861771	26.219431	65.775361
1489.728892	13.368236	65.780366
1488.320520	22.836237	65.785370
1487.561645	20.739867	65.790375
1487.435340	18.423124	65.795380
1486.563907	21.688872	65.800385
1485.667023	25.021742	65.805390
1484.860710	33.343837	65.810394
1484.540735	15.214408	65.815399
1484.139288	23.033770	65.820404
1482.865634	22.837413	65.825409
1482.324113	16.237472	65.830414
1481.653750	24.769766	65.835418
1481.183867	20.788766	65.840423
1480.537695	23.725408	65.845428
1479.581006	32.035131	65.850433
1479.600436	23.157256	65.855438
1478.856032	27.770022	65.860442
1477.924028	23.536036	65.865447
1477.057740	26.547083	65.870452
1476.144165	22.972482	65.875457
1475.979546	12.901738	65.880462
1475.322351	25.746432	65.885466
1474.257903	16.064689	65.890471
1473.666448	13.142212	65.895476
1473.319158	27.125088	65.900481
1472.782972	20.570031	65.905486
1471.521197	17.437118	65.910490
1471.197175	15.423032	65.915495
1470.572497	15.667587	65.920500
1470.006845	20.863796	65.925505
1469.395925	21.383705	65.930510
1467.941612	36.193795	65.935514
1467.845274	32.585509	65.940519
1467.381346	25.241539	65.945524
1466.982340	31.299082	65.950529
1465.851682	18.961267	65.955534
1465.002138	24.035440	65.960538
1464.213097	23.131302	65.965543
1463.983055	9.760976	65.970548
1463.644373	18.188518	65.975553
1462.824520	24.243557	65.980558
1461.986197	16.691014	65.985562
1461.534222	14.861266	65.990567
1460.568112	21.499359	65.995572
1459.519765	20.500817	66.000577
1459.185967	19.682024	66.005582
1458.642038	24.321280	66.010586
1458.417384	20.186195	66.015591
1457.572581	15.662398	66.020596
1456.813532	25.878764	66.025601
1456.127720	21.372275	66.030606
1455.571475	19.234250	66.035610
1454.561336	13.175567	66.040615
1454.071551	14.653927	66.045620
1453.486561	12.621395	66.050625
1453.044386	12.127330	66.055630
1451.691835	19.530154	66.060634
1451.023070	22.137659	66.065639
1451.061934	16.713342	66.070644
1450.077775	26.596484	66.075649
1449.599241	14.776352	66.080654
1448.470261	18.737470	66.085658
1447.983931	21.842677	66.090663
1447.754586	19.253735	66.095668
1446.637631	32.953668	66.100673
1445.901016	17.960758	66.105678
1445.209244	23.807790	66.110682
1444.876449	25.868322	66.115687
1444.809689	14.719175	66.120692
1443.533379	25.301601	66.125697
1442.873586	16.858109	66.130702
1442.009453	21.278602	66.135706
1441.515564	10.418115	66.140711
1440.655318	13.929675	66.145716
1439.919900	21.382654	66.150721
1439.596777	14.394782	66.155726
1439.070803	16.776171	66.160730
1438.325833	15.125456	66.165735
1437.416117	11.676414	66.170740
1436.824966	15.359670	66.175745
1436.394368	12.302829	66.180750
1435.370015	10.611365	66.185754
1434.935566	13.396095	66.190759
1434.591431	12.809181	66.195764
1433.962987	12.802035	66.200769
1433.222312	12.133068	66.205774
1431.975637	17.082711	66.210778
1431.605192	10.435097	66.215783
1430.921954	11.527897	66.220788
1429.790039	8.990949	66.225793
1429.180804	15.914522	66.230798
1428.456341	19.896510	66.235802
1428.275691	14.341505	66.240807
1428.101364	13.484755	66.245812
1427.246748	16.039804	66.250817
1426.509707	17.368236	66.255822
1425.657798	17.697803	66.260826
1425.225895	12.326234	66.265831
1424.321265	11.233903	66.270836
1423.338276	25.835048	66.275841
1423.352461	17.446865	66.280846
1422.839571	11.269741	66.285850
1421.818125	17.738446	66.290855
1420.768578	7.207556	66.295860
1420.290176	23.275470	66.300865
1419.864640	8.282024	66.305870
1418.738234	22.983232	66.310874
1417.876747	14.932925	66.315879
1417.941124	10.565832	66.320884
1417.242972	22.563919	66.325889
1416.522878	17.537773	66.330894
1415.374127	13.997424	66.335898
1414.853899	14.638547	66.340903
1414.307846	9.102202	66.345908
1413.835911	23.473886	66.350913
1413.574079	10.608512	66.355918
1412.289187	26.557038	66.360922
1412.231113	25.240270	66.365927
1411.216728	15.542718	66.370932
1410.025969	13.030901	66.375937
1409.436006	16.952091	66.380942
1408.764784	17.382252	66.385946
1408.713885	8.920842	66.390951
1408.584846	17.685644	66.395956
1407.184735	12.772320	66.400961
1406.726338	9.770366	66.405966
1406.074630	17.273121	66.410970
1404.763246	16.986608	66.415975
1404.320847	11.479519	66.420980
1403.499542	15.297134	66.425985
1403.231981	11.763383	66.430990
1402.809270	21.120483	66.435994
1402.077865	14.727364	66.440999
1401.215001	17.608580	66.446004
1400.581051	18.723515	66.451009
1400.383224	19.390666	66.456014
1398.918121	19.983287	66.461018
1398.071091	10.694378	66.466023
1397.788051	14.494244	66.471028
1397.360667	18.544134	66.476033
1397.151225	18.818898	66.481038
1395.689885	17.485487	66.486042
1395.352555	24.113542	66.491047
1395.195368	9.140526	66.496052
1393.782996	25.492515	66.501057
1392.714296	19.479435	66.506062
1392.257459	21.014069	66.511066
1391.895811	18.577049	66.516071
1391.881107	12.377515	66.521076
1390.752225	14.416359	66.526081
1390.391674	14.666258	66.531086
1389.386443	16.165061	66.536090
1388.316866	9.051429	66.541095
1387.915753	9.333006	66.546100
1386.982303	12.558178	66.551105
1387.145456	9.927356	66.556110
1386.157925	18.775003	66.561114
1385.280136	19.595969	66.566119
1384.515937	21.455424	66.571124
1384.160041	19.020645	66.576129
1383.589294	15.091971	66.581134
1382.343030	16.987053	66.586138
1381.685976	15.387035	66.591143
1381.377579	22.906188	66.596148
1381.182164	14.376288	66.601153
1379.961885	22.232776	66.606158
1379.189494	16.070103	66.611162
1378.471402	17.617883	66.616167
1378.050337	18.388329	66.621172
1377.921231	10.541741	66.626177
1377.225714	13.885211	66.631182
1375.916220	16.112042	66.636186
1375.190414	17.585356	66.641191
1374.955029	10.679745	66.646196
1373.631427	25.628354	66.651201
1373.331486	12.295965	66.656206
1372.888233	13.822135	66.661210
1372.660404	10.986961	66.666215
1371.931673	19.399241	66.671220
1370.884703	27.254993	66.676225
1370.513126	7.061725	66.681230
1369.108704	22.912569	66.686234
1368.705878	24.012850	66.691239
1368.053679	18.256847	66.696244
1367.223051	18.529434	66.701249
1367.255515	14.706725	66.706254
1366.002529	12.118090	66.711258
1365.307996	13.441357	66.716263
1364.909299	14.506289	66.721268
1364.221319	15.215089	66.726273
1363.983218	1.286265	66.731278
1362.815102	23.404115	66.736282
1362.051518	17.072894	66.741287
1361.859480	18.358861	66.746292
1360.835845	21.995767	66.751297
1359.994302	16.536367	66.756302
1359.204046	19.618940	66.761306
1358.661357	24.210706	66.766311
1358.614025	10.995861	66.771316
1357.896148	25.408221	66.776321
1356.920690	13.173534	66.781326
1356.192669	17.531413	66.786330
1355.608439	17.455757	66.791335
1355.482556	15.927424	66.796340
1354.233039	24.375189	66.801345
1353.856629	10.952463	66.806350
1353.004214	8.382159	66.811354
1352.167495	14.297978	66.816359
1351.639471	7.878857	66.821364
1350.668584	16.703366	66.826369
1350.401960	13.767130	66.831374
1350.007214	20.699199	66.836378
1349.016739	20.134621	66.841383
1348.294254	6.863109	66.846388
1347.622328	13.771429	66.851393
1347.572393	12.571641	66.856398
1346.463921	16.491692	66.861402
1345.967596	20.391700	66.866407
1345.657111	12.581835	66.871412
1344.261186	26.483831	66.876417
1343.720074	14.504949	66.881422
1343.272473	18.419289	66.886426
1342.532208	22.206693	66.891431
1341.663113	8.412870	66.896436
1340.863010	24.711698	66.901441
1340.520596	18.770839	66.906446
1339.894779	24.733563	66.911450
1339.386718	22.256749	66.916455
1338.706817	18.361208	66.921460
1337.666910	27.680818	66.926465
1337.372210	20.177520	66.931470
1335.892829	20.458636	66.936474
1335.247116	21.237994	66.941479
1335.354371	21.948111	66.946484
1334.415349	23.605141	66.951489
1334.174680	21.092129	66.956494
1332.977357	18.363776	66.961498
1332.127443	31.428360	66.966503
1331.904764	21.513520	66.971508
1331.072794	22.907531	66.976513
1331.062957	7.486913	66.981518
1329.609232	27.306863	66.986522
1328.883231	24.478350	66.991527
1328.874913	20.403507	66.996532
1328.314141	20.316243	67.001537
1327.369231	14.840174	67.006542
1326.398446	17.563531	67.011546
1326.160143	22.032795	67.016551
1325.690766	13.745152	67.021556
1324.298006	29.357626	67.026561
1323.843135	22.671413	67.031566
1323.663053	18.328991	67.036570
1322.636822	19.503155	67.041575
1322.087333	16.004774	67.046580
1321.226023	14.803093	67.051585
1320.823211	21.674947	67.056590
1319.384395	22.167240	67.061594
1318.857606	23.370813	67.066599
1318.442652	10.193920	67.071604
1318.032024	23.959781	67.076609
1318.055357	14.106762	67.081614
1316.797871	23.353735	67.086618
1316.017882	22.416667	67.091623
1315.759088	14.541819	67.096628
1314.386542	22.625964	67.101633
1313.616498	11.602843	67.106638
1313.487072	21.703364	67.111642
1313.050329	21.717808	67.116647
1312.533222	24.414775	67.121652
1311.015217	20.356023	67.126657
1310.593730	20.215080	67.131662
1310.079104	18.546707	67.136666
1309.102212	19.542724	67.141671
1308.784074	17.874651	67.146676
1307.620718	21.071748	67.151681
1307.406576	11.928259	67.156686
1306.972452	18.548051	67.161690
1306.418272	25.973822	67.166695
1305.292709	18.454394	67.171700
1304.658046	28.756669	67.176705
1304.514743	18.341946	67.181710
1303.594069	24.144975	67.186714
1302.716868	20.526814	67.191719
1301.965601	11.542838	67.196724
1301.856403	17.057581	67.201729
1301.070451	26.524481	67.206734
1300.223283	14.015540	67.211738
1299.174925	16.730739	67.216743
1299.032026	15.014306	67.221748
1298.273211	16.877660	67.226753
1297.288357	12.078151	67.231758
1296.617508	21.449479	67.236762
1296.759409	13.029965	67.241767
1295.297353	21.826930	67.246772
1294.414093	23.128183	67.251777
1294.036873	10.566609	67.256782
1293.657662	12.804842	67.261786
1293.117778	16.014780	67.266791
1292.628085	17.595654	67.271796
1291.589220	21.517277	67.276801
1291.169465	20.702712	67.281806
1290.447498	17.651225	67.286810
1289.266960	19.829210	67.291815
1289.116037	12.304643	67.296820
1288.473509	19.752344	67.301825
1287.608900	3.401635	67.306830
1286.753850	29.628097	67.311834
1285.973671	16.212813	67.316839
1285.817288	10.764356	67.321844
1285.157187	25.637464	67.326849
1284.206954	15.032504	67.331854
1283.430548	17.627201	67.336858
1282.633849	15.008638	67.341863
1282.752304	10.468949	67.346868
1281.538484	18.527870	67.351873
1280.727556	15.783840	67.356878
1280.443524	18.345983	67.361882
1279.866230	9.485742	67.366887
1279.389992	9.974820	67.371892
1278.223310	16.726857	67.376897
1278.031471	1.765693	67.381902
1277.035128	22.654629	67.386906
1276.260283	14.264183	67.391911
1275.601112	6.093466	67.396916
1274.980786	19.060046	67.401921
1274.813704	6.278991	67.406926
1273.627319	15.040015	67.411930
1272.763182	14.237764	67.416935
1272.523527	8.493471	67.421940
1271.912886	12.386434	67.426945
1271.365828	11.092228	67.431950
1270.171227	13.743959	67.436954
1269.853200	15.144580	67.441959
1269.430787	9.156536	67.446964
1268.350403	14.866697	67.451969
1267.544371	11.021196	67.456974
1266.952132	10.626717	67.461978
1266.351652	8.462658	67.466983
1266.271380	16.073270	67.471988
1265.166187	6.087467	67.476993
1264.482533	17.734765	67.481998
1264.087417	10.092913	67.487002
1263.176953	11.374848	67.492007
1262.304606	4.512191	67.497012
1261.490036	11.176706	67.502017
1261.600813	15.144196	67.507022
1260.943174	14.058383	67.512026
1259.877827	14.445596	67.517031
1259.484780	16.709689	67.522036
1258.782694	14.165976	67.527041
1257.927633	8.434383	67.532046
1256.672202	16.011081	67.537050
1255.848578	16.605862	67.542055
1255.829100	10.230482	67.547060
1255.306124	12.223502	67.552065
1255.282051	5.990778	67.557070
1254.037073	15.125397	67.562074
1253.036690	10.156492	67.567079
1252.818695	4.503375	67.572084
1251.804329	16.394067	67.577089
1250.945587	12.585338	67.582094
1250.336488	6.847755	67.587098
1250.084514	9.907842	67.592103
1249.781543	12.124497	67.597108
1248.549504	13.508031	67.602113
1248.177743	10.227411	67.607118
1247.516109	7.853887	67.612122
1246.698101	14.280838	67.617127
1246.406536	10.385079	67.622132
1245.220871	10.982238	67.627137
1244.881599	4.364403	67.632142
1243.719806	18.405817	67.637146
1242.938773	-0.161125	67.642151
1242.650200	4.440709	67.647156
1242.261334	7.263947	67.652161
1241.713742	2.617284	67.657166
1240.685631	6.321172	67.662170
1240.023755	7.468970	67.667175
1239.533625	-1.160688	67.672180
1238.936898	14.725763	67.677185
1238.102872	-4.712671	67.682190
1237.368851	10.919645	67.687194
1236.663078	7.315254	67.692199
1235.843629	-3.195350	67.697204
1234.865660	12.005834	67.702209
1234.563085	0.654535	67.707214
1234.299304	-1.906825	67.712218
1233.686283	6.468151	67.717223
1233.173840	4.406794	67.722228
1232.099003	-0.338950	67.727233
1231.790864	8.526856	67.732238
1230.905203	9.741780	67.737242
1229.837057	7.283095	67.742247
1229.590481	10.279248	67.747252
1229.083520	4.894431	67.752257
1228.375207	5.201229	67.757262
1227.775000	0.398937	67.762266
1226.687531	12.376949	67.767271
1226.298543	6.774680	67.772276
1225.026765	12.281905	67.777281
1224.496810	2.712425	67.782286
1223.979025	6.937554	67.787290
1223.621365	10.284104	67.792295
1223.319601	9.520174	67.797300
1222.002887	1.957080	67.802305
1221.512496	7.458319	67.807310
1221.231897	6.862909	67.812314
1220.461520	11.394708	67.817319
1219.644743	8.760439	67.822324
1219.045923	13.690728	67.827329
1218.158136	0.276833	67.832334
1217.879474	2.954817	67.837338
1217.110278	15.642303	67.842343
1216.653328	5.209672	67.847348
1215.608840	11.697876	67.852353
1214.615751	15.314205	67.857358
1213.827786	11.842737	67.862362
1213.392514	16.303904	67.867367
1213.035672	17.833704	67.872372
1212.590849	16.318253	67.877377
1211.889736	13.902131	67.882382
1210.981206	6.576901	67.887386
1210.231308	14.254572	67.892391
1210.157050	10.321108	67.897396
1208.966445	7.099749	67.902401
1208.131753	19.318269	67.907406
1207.694248	13.554985	67.912410
1207.251725	12.919096	67.917415
1206.409193	12.860896	67.922420
1205.417689	11.077574	67.927425
1205.128656	12.155051	67.932430
1204.503440	2.636995	67.937434
1203.662065	17.584662	67.942439
1203.046178	3.857876	67.947444
1202.213553	9.277927	67.952449
1201.912888	-0.517239	67.957454
1201.256352	7.695932	67.962458
1200.337592	11.637908	67.967463
1199.810228	10.682780	67.972468
1199.066440	11.673306	67.977473
1198.939908	7.628311	67.982478
1197.989061	2.579017	67.987482
1197.058188	8.795272	67.992487
1196.537600	13.703663	67.997492
1195.419277	10.212200	68.002497
1194.912666	16.261642	68.007502
1194.320050	4.518089	68.012506
1193.514972	22.194382	68.017511
1193.529044	5.282943	68.022516
1192.466005	12.876377	68.027521
1191.820984	5.567597	68.032526
1191.116211	12.575785	68.037530
1190.724030	11.346853	68.042535
1190.556166	5.491810	68.047540
1189.206599	26.492131	68.052545
1188.791742	12.533103	68.057550
1187.595932	8.803235	68.062554
1186.649363	24.035717	68.067559
1186.654423	9.625142	68.072564
1186.092864	9.747766	68.077569
1185.418549	22.082710	68.082574
1184.217274	16.764166	68.087578
1183.338057	24.169105	68.092583
1183.269247	10.765319	68.097588
1182.737396	12.989995	68.102593
1182.340529	4.025403	68.107598
1181.240545	20.013974	68.112602
1180.844587	9.678883	68.117607
1180.299276	11.863123	68.122612
1179.067732	22.731837	68.127617
1178.639190	7.868259	68.132622
1178.005851	5.884487	68.137626
1177.567253	19.274753	68.142631
1176.714298	16.695135	68.147636
1175.697332	11.060285	68.152641
1175.395490	-0.578116	68.157646
1174.790369	5.515376	68.162650
1173.862531	7.369375	68.167655
1173.374161	9.446791	68.172660
1172.803537	9.755360	68.177665
1172.123814	14.892487	68.182670
1171.347085	5.299192	68.187674
1170.420895	11.508403	68.192679
1170.265595	8.340026	68.197684
1169.600325	13.284047	68.202689
1168.692693	12.457211	68.207694
1167.920710	11.192493	68.212698
1166.763416	20.012010	68.217703
1166.743864	-0.476851	68.222708
1166.321756	4.710765	68.227713
1165.539641	11.382758	68.232718
1164.781541	-1.597580	68.237722
1164.421011	8.809333	68.242727
1164.101646	-4.740665	68.247732
1162.574522	6.875208	68.252737
1161.935620	9.096413	68.257742
1161.701548	6.960837	68.262746
1160.472178	8.591566	68.267751
1159.854408	15.981734	68.272756
1159.093816	19.215759	68.277761
1158.848054	8.159785	68.282766
1158.623816	8.481075	68.287770
1157.714512	12.776369	68.292775
1156.935475	9.901157	68.297780
1155.997567	7.371329	68.302785
1155.723503	20.000580	68.307790
1154.582715	5.204561	68.312794
1153.612977	10.039315	68.317799
1153.649641	7.218872	68.322804
1153.302274	19.407203	68.327809
1152.481308	7.617980	68.332814
1151.635869	8.753995	68.337818
1150.851160	12.668359	68.342823
1150.638081	7.870746	68.347828
1149.251612	9.792967	68.352833
1148.544916	15.087351	68.357838
1148.195603	11.039945	68.362842
1147.727079	6.106345	68.367847
1147.257076	-0.919599	68.372852
1146.088449	25.333082	68.377857
1145.560599	12.420197	68.382862
1145.476771	16.229397	68.387866
1144.353979	13.943440	68.392871
1143.863822	16.407493	68.397876
1142.705276	15.659998	68.402881
1142.322188	8.296957	68.407886
1141.839933	10.570521	68.412890
1140.646465	10.725853	68.417895
1140.439750	8.699467	68.422900
1139.652197	17.638378	68.427905
1138.573220	12.221561	68.432910
1138.034044	14.035833	68.437914
1137.062706	20.851472	68.442919
1137.383572	8.636221	68.447924
1137.022164	9.329408	68.452929
1136.072487	13.068168	68.457934
1135.194150	17.126737	68.462938
1134.643887	7.886936	68.467943
1133.573951	5.554732	68.472948
1132.802397	8.276428	68.477953
1132.432060	8.270880	68.482958
1132.392665	7.329616	68.487962
1131.474316	11.963819	68.492967
1130.705452	3.813756	68.497972
1129.506716	9.620058	68.502977
1128.594965	1.189954	68.507982
1128.256985	11.019281	68.512986
1127.640253	5.904258	68.517991
1127.743213	9.783094	68.522996
1126.752512	11.358530	68.528001
1125.902866	10.438910	68.533006
1125.064849	11.726715	68.538010
1124.379037	1.051401	68.543015
1123.649950	13.212134	68.548020
1122.782998	13.766541	68.553025
1122.100683	17.629935	68.558030
1121.836851	11.140469	68.563034
1121.371927	20.709302	68.568039
1120.759520	3.515909	68.573044
1119.393117	21.942225	68.578049
1119.021247	14.405517	68.583054
1118.931485	17.938122	68.588058
1118.098255	12.657266	68.593063
1117.300509	9.980582	68.598068
1116.479903	14.697013	68.603073
1115.955836	12.951339	68.608078
1115.058666	4.242957	68.613082
1113.836613	17.713686	68.618087
1113.544807	7.183856	68.623092
1112.690846	12.306132	68.628097
1112.962648	11.173445	68.633102
1112.601333	9.346692	68.638106
1111.573805	16.721621	68.643111
1111.028068	5.104680	68.648116
1110.050444	8.726470	68.653121
1109.079005	14.753667	68.658126
1108.652771	7.260305	68.663130
1107.913830	20.233154	68.668135
1107.501106	0.325654	68.673140
1106.129651	11.743334	68.678145
1105.500912	5.775534	68.683150
1105.157775	4.923586	68.688154
1104.913424	23.464739	68.693159
1104.578719	9.220183	68.698164
1103.209306	15.730149	68.703169
1102.698303	15.940942	68.708174
1102.463869	2.743293	68.713178
1101.142480	13.310934	68.718183
1100.575438	3.692199	68.723188
1100.129380	12.652487	68.728193
1099.692392	2.916873	68.733198
1098.718398	17.880922	68.738202
1097.656907	8.753990	68.743207
1097.361917	1.242911	68.748212
1096.754807	12.725090	68.753217
1096.202529	15.443456	68.758222
1095.396195	5.536362	68.763226
1094.943829	20.983556	68.768231
1094.881799	12.244835	68.773236
1093.934242	9.497373	68.778241
1093.221391	10.924548	68.783246
1092.365511	6.140885	68.788250
1090.725946	10.986017	68.793255
1090.006568	4.988486	68.798260
1089.552407	9.556748	68.803265
1089.102186	3.205749	68.808270
1089.228054	0.194503	68.813274
1088.296917	4.826021	68.818279
1087.571832	1.923328	68.823284
1086.752070	14.916917	68.828289
1086.503810	12.802529	68.833294
1085.702079	15.823924	68.838298
1084.465555	16.320440	68.843303
1083.994137	1.242951	68.848308
1083.855334	12.860368	68.853313
1083.161398	12.333879	68.858318
1082.279376	13.817929	68.863322
1081.622233	10.186927	68.868327
1081.104233	8.118603	68.873332
1079.979768	12.881803	68.878337
1079.341989	6.552756	68.883342
1078.994449	9.995480	68.888346
1078.165151	10.271103	68.893351
1077.452230	3.260164	68.898356
1076.682964	8.562938	68.903361
1075.948721	10.960176	68.908366
1075.845535	5.154783	68.913370
1075.363121	12.976009	68.918375
1074.535794	1.630955	68.923380
1073.610264	16.492682	68.928385
1073.176401	9.582427	68.933390
1072.415033	4.813700	68.938394
1071.089410	14.803296	68.943399
1070.837028	3.499244	68.948404
1070.142976	13.773141	68.953409
1069.924223	12.194947	68.958414
1069.057393	9.363692	68.963418
1068.009725	12.455754	68.968423
1067.959550	5.588542	68.973428
1067.370788	11.755145	68.978433
1066.162446	4.472943	68.983438
1065.461836	-1.284715	68.988442
1064.722240	16.124130	68.993447
1064.615925	14.453934	68.998452
1063.545739	13.949458	69.003457
1062.853922	10.368132	69.008462
1062.407269	7.411691	69.013466
1061.767979	14.639721	69.018471
1061.529719	10.445357	69.023476
1060.386664	12.043478	69.028481
1060.055093	6.220803	69.033486
1059.647600	5.235599	69.038490
1057.899890	10.471685	69.043495
1057.468115	-2.622017	69.048500
1056.639679	3.355635	69.053505
1056.535422	17.150023	69.058510
1056.342527	10.474245	69.063514
1054.974178	17.957028	69.068519
1054.526834	10.514344	69.073524
1054.049030	3.415548	69.078529
1052.869634	15.599047	69.083534
1052.199099	6.473022	69.088538
1051.545195	20.440006	69.093543
1051.362230	9.254218	69.098548
1050.790493	0.255981	69.103553
1049.591176	11.092799	69.108558
1048.943979	11.202269	69.113562
1048.417318	2.015514	69.118567
1048.357485	7.937127	69.123572
1047.448777	12.434207	69.128577
1046.502398	8.399806	69.133582
1046.277268	7.874439	69.138586
1045.022585	12.899638	69.143591
1044.492598	6.301146	69.148596
1044.163065	9.211162	69.153601
1043.675873	8.964025	69.158606
1042.377671	11.253875	69.163610
1041.719784	8.422505	69.168615
1041.244425	7.591601	69.173620
1041.089940	5.891224	69.178625
1039.465824	11.159699	69.183630
1039.290313	4.799700	69.188634
1038.692698	10.327484	69.193639
1038.069042	4.557590	69.198644
1037.115974	7.043265	69.203649
1036.312218	16.046275	69.208654
1035.911996	-0.800794	69.213658
1035.489036	3.188509	69.218663
1035.262386	7.469851	69.223668
1034.244055	14.163686	69.228673
1033.510030	15.956939	69.233678
1032.691717	8.671049	69.238682
1031.268761	19.403112	69.243687
1031.291817	4.969203	69.248692
1030.798151	15.219112	69.253697
1030.230029	10.159461	69.258702
1029.678933	10.873379	69.263706
1028.369194	20.322738	69.268711
1028.211265	4.056851	69.273716
1027.569209	8.908899	69.278721
1026.305374	8.253901	69.283726
1025.830010	10.606811	69.288730
1025.014097	11.515823	69.293735
1024.912330	10.429946	69.298740
1024.503480	9.802925	69.303745
1023.718287	9.978511	69.308750
1022.782966	7.386824	69.313754
1022.232100	5.322166	69.318759
1021.525602	2.020729	69.323764
1020.387526	5.247038	69.328769
1019.995194	4.987967	69.333774
1019.527110	9.340837	69.338778
1018.654434	5.950724	69.343783
1017.592715	7.397153	69.348788
1016.931836	5.567615	69.353793
1016.656284	8.483237	69.358798
1016.498275	9.071541	69.363802
1016.222431	12.430327	69.368807
1015.634784	7.958826	69.373812
1014.618038	-1.143636	69.378817
1013.291416	16.156764	69.383822
1012.890301	4.480578	69.388826
1012.055049	11.910100	69.393831
1011.837183	10.366464	69.398836
1010.341874	3.563605	69.403841
1009.806506	12.131262	69.408846
1009.571643	0.452284	69.413850
1008.691834	25.294997	69.418855
1008.674108	4.574069	69.423860
1007.396403	13.441181	69.428865
1006.690747	4.648762	69.433870
1006.202897	10.551742	69.438874
1005.917089	9.236532	69.443879
1005.035832	5.984982	69.448884
1004.108507	5.706956	69.453889
1003.451405	0.109549	69.458894
1003.354454	-5.774092	69.463898
1002.321823	11.807531	69.468903
1002.000436	2.528207	69.473908
1001.226521	0.664619	69.478913
1000.111825	15.751996	69.483918
999.589987	5.736601	69.488922
998.596852	18.592216	69.493927
998.643276	4.638710	69.498932
997.986861	11.655012	69.503937
996.924047	10.053429	69.508942
996.361149	7.814075	69.513946
995.501637	15.023540	69.518951
995.243309	3.665258	69.523956
994.198182	11.806254	69.528961
993.330537	12.177891	69.533966
993.312525	7.366609	69.538970
992.704421	13.619880	69.543975
991.553490	9.460356	69.548980
990.764287	9.810051	69.553985
990.570611	-1.724090	69.558990
990.122657	7.550313	69.563994
988.601186	10.429214	69.568999
988.058701	4.537613	69.574004
987.825683	3.735968	69.579009
987.571296	17.366581	69.584014
986.556583	6.122340	69.589018
985.389838	9.913033	69.594023
985.383314	3.166617	69.599028
984.732622	4.700622	69.604033
983.614036	6.083575	69.609038
983.417301	-1.419460	69.614042
982.477995	10.490895	69.619047
982.060132	8.862391	69.624052
980.991126	9.406418	69.629057
979.915869	6.441206	69.634062
980.042550	4.525790	69.639066
979.521372	9.095268	69.644071
978.641825	5.985378	69.649076
977.611230	0.963062	69.654081
977.364157	7.871657	69.659086
976.922987	-0.491330	69.664090
975.491362	10.019784	69.669095
975.257542	11.083769	69.674100
974.589557	4.245486	69.679105
974.254317	10.488456	69.684110
973.219610	2.465909	69.689114
972.215923	9.944318	69.694119
972.343144	3.487275	69.699124
971.082353	11.987441	69.704129
970.256690	9.603827	69.709134
969.916052	4.862806	69.714138
969.075616	16.211821	69.719143
969.011428	5.272076	69.724148
967.935239	5.099751	69.729153
966.883843	9.444521	69.734158
966.811233	6.936353	69.739162
966.108137	9.434318	69.744167
965.174594	7.842141	69.749172
964.703596	7.612943	69.754177
963.934481	8.077719	69.759182
963.612772	6.850227	69.764186
962.510422	8.642183	69.769191
961.905454	7.877648	69.774196
961.374667	4.221848	69.779201
960.775902	6.438288	69.784206
960.131245	7.048839	69.789210
959.420813	10.814242	69.794215
958.944402	9.538829	69.799220
957.976841	2.030721	69.804225
956.922622	5.201135	69.809230
956.574358	8.973563	69.814234
955.986759	7.912958	69.819239
955.454916	13.315177	69.824244
954.826528	3.542252	69.829249
953.783610	9.421601	69.834254
953.484747	5.165936	69.839258
953.121842	10.721041	69.844263
952.075271	1.741624	69.849268
951.490821	6.455211	69.854273
950.664778	14.107208	69.859278
950.939979	3.010962	69.864282
949.264045	16.036737	69.869287
948.673537	13.246711	69.874292
948.215581	-1.088561	69.879297
947.394655	16.777930	69.884302
946.662465	9.692832	69.889306
945.572720	8.677442	69.894311
945.423476	3.532239	69.899316
945.285640	4.609337	69.904321
944.343495	6.369499	69.909326
943.514607	1.076986	69.914330
942.989246	8.484019	69.919335
942.006268	16.466915	69.924340
940.843737	13.211261	69.929345
940.232763	18.599268	69.934350
940.219090	2.278911	69.939354
939.765595	6.588470	69.944359
939.373690	11.602576	69.949364
938.404433	16.153480	69.954369
937.371524	12.624894	69.959374
937.361503	6.853575	69.964378
936.283310	18.756087	69.969383
935.603892	9.119016	69.974388
935.104524	8.115338	69.979393
934.410877	9.533191	69.984398
933.464527	9.119450	69.989402
932.469708	15.353847	69.994407
932.150252	6.496845	69.999412
932.131616	13.779091	70.004417
931.343508	2.478323	70.009422
930.459798	4.911998	70.014426
929.139513	9.509302	70.019431
928.885400	14.845252	70.024436
928.124416	8.244129	70.029441
927.355641	14.690133	70.034446
927.039774	1.652139	70.039450
926.615249	12.231667	70.044455
926.222655	1.646961	70.049460
924.777847	9.433698	70.054465
924.269530	10.296945	70.059470
924.003922	15.128533	70.064474
922.845763	14.759540	70.069479
922.390701	9.161543	70.074484
921.326013	5.727908	70.079489
921.157659	14.117325	70.084494
920.644420	3.288473	70.089498
919.489692	11.989396	70.094503
919.198143	8.517880	70.099508
918.926654	5.574595	70.104513
917.895694	16.015671	70.109518
917.126388	18.407493	70.114522
916.301948	14.667548	70.119527
915.993723	8.642493	70.124532
914.815219	11.991973	70.129537
914.217899	19.131351	70.134542
913.876110	14.494597	70.139546
913.348089	9.406521	70.144551
912.428962	8.165302	70.149556
911.590386	3.623380	70.154561
910.914649	14.572465	70.159566
910.765633	-1.371536	70.164570
909.852165	16.050802	70.169575
908.912585	2.545956	70.174580
908.105909	8.452378	70.179585
907.743395	21.016852	70.184590
907.830923	14.629200	70.189594
906.424436	19.066774	70.194599
906.024921	1.123674	70.199604
905.725464	12.771376	70.204609
904.532749	11.195237	70.209614
903.741936	11.039023	70.214618
903.106703	11.384742	70.219623
902.624674	12.735811	70.224628
901.611011	20.036065	70.229633
900.684561	5.893630	70.234638
900.420444	14.099595	70.239642
900.099676	10.438770	70.244647
899.548994	15.651611	70.249652
898.344320	24.858806	70.254657
897.997687	13.399477	70.259662
897.525585	10.868159	70.264666
896.815630	16.879041	70.269671
895.925983	11.951020	70.274676
895.298145	12.896372	70.279681
894.618984	11.840892	70.284686
894.339922	6.844085	70.289690
893.524282	18.424133	70.294695
892.814502	11.835372	70.299700
892.194868	18.921535	70.304705
890.516297	11.681149	70.309710
890.058868	12.925805	70.314714
889.412088	12.932750	70.319719
889.405392	7.695481	70.324724
888.891523	10.371503	70.329729
888.442641	3.003226	70.334734
887.692641	12.257903	70.339738
886.853080	22.424108	70.344743
886.133814	11.711627	70.349748
885.157469	9.645332	70.354753
884.353199	11.500266	70.359758
884.010466	7.171170	70.364762
883.574347	15.114357	70.369767
883.370636	2.331332	70.374772
882.257429	14.138506	70.379777
881.675168	12.897301	70.384782
880.558333	-3.785198	70.389786
879.645439	16.161704	70.394791
879.127488	4.056307	70.399796
878.831465	9.969773	70.404801
878.430181	7.200113	70.409806
878.085379	7.884384	70.414810
876.922902	14.033521	70.419815
876.170364	13.625224	70.424820
875.590073	5.112518	70.429825
874.501733	21.996586	70.434830
874.368736	10.285648	70.439834
873.371362	16.716010	70.444839
872.778382	1.479752	70.449844
871.793801	16.365110	70.454849
871.087926	12.686735	70.459854
871.361498	5.679708	70.464858
870.319482	12.394713	70.469863
869.698110	7.430314	70.474868
869.191735	1.955615	70.479873
868.435275	15.593590	70.484878
867.287836	5.263076	70.489882
866.561707	16.235958	70.494887
866.150287	2.913573	70.499892
865.599204	5.231252	70.504897
864.836796	3.182955	70.509902
864.052399	-0.780955	70.514906
863.288234	12.828284	70.519911
863.095978	4.991822	70.524916
862.630345	1.499139	70.529921
861.452696	13.526306	70.534926
861.016170	2.412456	70.539930
860.329602	6.658199	70.544935
859.778884	3.513365	70.549940
858.866453	1.949409	70.554945
858.012287	6.076750	70.559950
857.977059	-2.289315	70.564954
857.095356	11.425362	70.569959
856.044520	3.233556	70.574964
855.581320	0.418563	70.579969
854.998095	7.610894	70.584974
854.841925	-9.137754	70.589978
853.508168	12.654899	70.594983
852.792435	3.040991	70.599988
852.533199	8.935987	70.604993
851.638769	11.696242	70.609998
850.608517	2.670125	70.615002
849.982769	7.565343	70.620007
849.332511	3.241049	70.625012
849.186344	9.051818	70.630017
848.952293	5.232123	70.635022
848.059449	6.863050	70.640026
847.024056	5.667169	70.645031
846.594656	4.226604	70.650036
846.026172	2.123793	70.655041
844.583065	11.092989	70.660046
844.399635	-0.802291	70.665050
843.727575	10.021639	70.670055
843.388831	10.313874	70.675060
842.338761	0.505610	70.680065
841.830988	5.957627	70.685070
841.477026	-12.096761	70.690074
840.542941	-0.444250	70.695079
839.317356	-7.594266	70.700084
839.132404	-3.575017	70.705089
838.934217	-2.988193	70.710094
837.996499	-3.111541	70.715098
837.108226	1.590502	70.720103
836.689956	4.967238	70.725108
835.795013	1.246433	70.730113
834.628990	13.932488	70.735118
833.947056	5.797089	70.740122
833.638791	-4.206510	70.745127
833.418224	1.869983	70.750132
832.987907	3.739524	70.755137
832.009202	-0.352716	70.760142
831.536762	4.776718	70.765146
831.088729	2.593238	70.770151
830.326217	1.615698	70.775156
829.506304	-0.767203	70.780161
828.576992	13.048097	70.785166
827.619219	-6.640065	70.790170
826.628172	7.408979	70.795175
826.177687	-4.629862	70.800180
825.983152	10.227514	70.805185
825.373295	-4.457264	70.810190
825.022766	0.165495	70.815194
823.939603	0.543110	70.820199
823.200715	-1.559378	70.825204
822.950192	-1.364760	70.830209
821.594006	9.765184	70.835214
820.766580	-3.401079	70.840218
820.703639	11.082121	70.845223
820.157853	-2.381280	70.850228
819.556799	9.808002	70.855233
818.558981	8.866343	70.860238
818.168445	3.680718	70.865242
817.281670	7.545186	70.870247
817.110449	5.637761	70.875252
815.991383	12.306703	70.880257
815.262101	4.368078	70.885262
815.177864	6.007495	70.890266
813.474058	7.549907	70.895271
813.106040	17.705719	70.900276
812.674321	9.437458	70.905281
811.989500	10.787708	70.910286
812.069449	-0.271145	70.915290
811.091576	3.257748	70.920295
810.025615	1.223096	70.925300
809.591994	-2.295170	70.930305
808.509380	13.504649	70.935310
808.011176	-3.383509	70.940314
807.190823	9.936641	70.945319
807.049808	1.830265	70.950324
806.246789	-3.070504	70.955329
804.956591	6.582405	70.960334
805.018946	-1.307189	70.965338
804.011923	8.772145	70.970343
803.781184	2.525048	70.975348
802.593302	-10.574359	70.980353
801.937816	12.523259	70.985358
801.814564	-1.477319	70.990362
800.779886	17.788830	70.995367
800.140995	4.633558	71.000372
799.477459	11.523300	71.005377
798.873337	6.869984	71.010382
798.713408	3.336536	71.015386
797.432407	5.959651	71.020391
796.752514	12.317421	71.025396
796.243092	4.460497	71.030401
795.547625	10.327170	71.035406
795.012698	2.193616	71.040410
794.051562	10.825921	71.045415
793.690523	9.868059	71.050420
793.219162	6.149226	71.055425
791.783409	11.619667	71.060430
791.590857	1.302770	71.065434
791.176182	9.947431	71.070439
790.383410	11.907793	71.075444
789.668310	-0.008494	71.080449
788.924647	11.585342	71.085454
788.818547	7.451979	71.090458
787.293593	12.835700	71.095463
786.799950	8.311454	71.100468
786.318487	3.252272	71.105473
785.806916	-0.053312	71.110478
784.954315	-0.690074	71.115482
784.033838	6.994338	71.120487
783.327655	-3.553019	71.125492
783.076786	6.544715	71.130497
782.755725	10.549368	71.135502
782.090285	6.858278	71.140506
781.102636	2.049986	71.145511
780.545908	7.265383	71.150516
779.312357	6.214614	71.155521
778.838562	9.966043	71.160526
778.638407	-6.102242	71.165530
778.174252	10.231472	71.170535
777.006827	2.928727	71.175540
776.290254	4.473270	71.180545
775.644501	7.452576	71.185550
775.087727	2.887923	71.190554
774.064897	-3.523222	71.195559
773.048360	4.020369	71.200564
772.828928	-5.066975	71.205569
772.278144	6.021501	71.210574
772.463483	6.375391	71.215578
771.307790	6.083345	71.220583
770.589826	4.838540	71.225588
770.022464	1.519765	71.230593
769.458361	3.151998	71.235598
768.717769	4.083792	71.240602
767.742984	6.495750	71.245607
767.329686	3.280179	71.250612
766.164588	2.478712	71.255617
765.425804	3.168949	71.260622
765.341215	1.064816	71.265626
764.584950	1.067146	71.270631
763.899673	5.948203	71.275636
763.068833	7.761672	71.280641
762.726319	-2.607035	71.285646
762.146025	-7.284629	71.290650
760.831636	9.386286	71.295655
760.021658	5.563676	71.300660
759.849225	-0.574425	71.305665
759.013353	6.429488	71.310670
759.075194	-0.091255	71.315674
758.063624	1.331527	71.320679
757.068789	7.059789	71.325684
757.036827	-1.883938	71.330689
756.072588	8.150752	71.335694
755.068164	3.722025	71.340698
754.311763	4.016110	71.345703
754.153274	5.178504	71.350708
753.392793	-6.867730	71.355713
752.077238	6.755188	71.360718
751.853636	4.039264	71.365722
751.342790	-4.489182	71.370727
750.958352	-10.587218	71.375732
750.060377	-3.294306	71.380737
749.351664	6.322820	71.385742
748.716896	-8.381611	71.390746
748.146135	3.473274	71.395751
747.194272	4.733593	71.400756
746.779227	-1.914648	71.405761
746.103576	5.812797	71.410766
745.695254	11.217458	71.415770
744.510822	7.873929	71.420775
744.001084	11.298356	71.425780
743.889482	-0.504262	71.430785
742.617959	7.073628	71.435790
741.912988	-6.214590	71.440794
741.321395	-1.047253	71.445799
740.785723	8.335749	71.450804
740.040685	-2.287405	71.455809
739.211222	3.837147	71.460814
738.796279	2.011110	71.465818
738.047458	3.313221	71.470823
737.394278	6.705294	71.475828
736.641890	-2.636230	71.480833
735.575470	9.267613	71.485838
735.550690	-1.900711	71.490842
735.077743	6.355846	71.495847
734.212919	-6.774457	71.500852
733.499778	-6.380022	71.505857
732.773160	-7.795321	71.510862
732.336783	-9.230021	71.515866
731.404786	2.862147	71.520871
730.633650	8.390803	71.525876
730.353594	-0.138115	71.530881
729.508543	1.284973	71.535886
728.875314	6.624520	71.540890
727.767555	3.440678	71.545895
727.529451	0.526798	71.550900
727.079862	-1.861411	71.555905
726.106624	6.072685	71.560910
725.287769	1.193390	71.565914
724.858340	5.325684	71.570919
724.246757	6.309489	71.575924
724.231439	-3.133613	71.580929
722.875556	7.794477	71.585934
722.104167	1.428475	71.590938
722.013833	-4.279576	71.595943
721.021838	0.017979	71.600948
720.142835	1.097977	71.605953
719.405199	12.780750	71.610958
719.150987	-0.287502	71.615962
718.061308	1.366923	71.620967
717.424099	5.407724	71.625972
717.164642	-0.942015	71.630977
716.508111	5.210203	71.635982
715.668607	-2.874829	71.640986
714.827904	5.684705	71.645991
714.151105	6.746703	71.650996
714.211892	-6.851079	71.656001
713.070259	11.831304	71.661006
712.316356	-9.827278	71.666010
711.791673	6.542876	71.671015
710.794981	0.780442	71.676020
710.299513	6.239980	71.681025
709.256034	-3.952451	71.686030
709.280425	7.952758	71.691034
708.864111	3.403605	71.696039
707.712939	0.792799	71.701044
707.051198	-2.381625	71.706049
706.426419	0.193818	71.711054
706.068860	5.434284	71.716058
705.033340	-0.713040	71.721063
704.515029	1.105877	71.726068
704.075146	-7.227277	71.731073
702.644433	8.709989	71.736078
702.216598	-4.283302	71.741082
701.724475	1.095280	71.746087
701.225629	0.608798	71.751092
700.913813	2.013222	71.756097
699.760245	4.370095	71.761102
699.177532	-4.873852	71.766106
698.079613	3.335565	71.771111
697.298087	-3.508195	71.776116
696.966974	-6.192799	71.781121
696.442485	1.327661	71.786126
696.561936	-4.844290	71.791130
695.305409	4.147303	71.796135
694.240466	4.425881	71.801140
693.941552	-1.345149	71.806145
693.247210	4.229633	71.811150
692.251137	3.910632	71.816154
691.735774	2.572092	71.821159
690.862913	-4.129391	71.826164
691.008267	3.541450	71.831169
689.940604	-3.121131	71.836174
689.089267	-0.433918	71.841178
688.831157	-6.271365	71.846183
688.317145	-4.697552	71.851188
687.016599	-7.920059	71.856193
686.274263	-4.896973	71.861198
686.118766	-6.912541	71.866202
685.324926	1.302076	71.871207
684.448548	-1.242089	71.876212
683.984327	-12.110196	71.881217
683.271617	-4.559767	71.886222
682.485158	-6.266713	71.891226
681.655135	1.240899	71.896231
680.755271	-1.490332	71.901236
680.281020	-3.316375	71.906241
679.971513	-6.572108	71.911246
679.654563	1.451459	71.916250
679.214346	1.157491	71.921255
678.268112	6.972656	71.926260
677.580420	-3.580757	71.931265
676.585870	-6.031986	71.936270
675.723417	-3.659960	71.941274
675.224417	-3.766375	71.946279
674.543597	-9.891315	71.951284
674.483686	-6.084356	71.956289
673.399020	0.869309	71.961294
672.768882	-0.545566	71.966298
672.279398	5.934867	71.971303
671.239486	1.898174	71.976308
670.625639	-1.960362	71.981313
669.552581	8.440178	71.986318
669.244920	-9.921141	71.991322
669.082805	-1.879654	71.996327
667.896968	-4.541688	72.001332
667.678826	-2.969255	72.006337
666.884836	-1.770315	72.011342
666.734557	-7.954504	72.016346
665.479727	-1.114087	72.021351
664.976481	0.331863	72.026356
664.476027	-2.450348	72.031361
663.198120	1.115336	72.036366
663.022592	-2.607997	72.041370
662.365465	-5.032529	72.046375
661.135588	-7.544046	72.051380
660.374048	-3.601706	72.056385
660.012699	-1.076086	72.061390
659.861761	-7.484092	72.066394
658.630890	-4.750625	72.071399
658.039432	3.231503	72.076404
657.538811	-11.603056	72.081409
657.119197	-3.498489	72.086414
656.562623	-7.621601	72.091418
655.348995	-8.746439	72.096423
654.767100	-2.886789	72.101428
654.300739	0.754665	72.106433
653.642517	-2.413995	72.111438
652.738581	-6.098601	72.116442
651.911253	5.008693	72.121447
651.896886	2.784576	72.126452
651.283317	6.044206	72.131457
650.046900	-3.685393	72.136462
649.179855	5.900194	72.141466
648.938265	-3.863250	72.146471
648.362354	4.081712	72.151476
647.124827	-10.097766	72.156481
646.602689	6.497484	72.161486
646.666261	-3.951630	72.166490
645.907245	7.398672	72.171495
645.176004	5.064792	72.176500
644.285738	-3.196625	72.181505
643.741617	-2.654044	72.186510
643.274092	1.575788	72.191514
642.280075	-3.767578	72.196519
641.450436	3.531832	72.201524
641.222409	-5.776463	72.206529
639.980884	-6.392238	72.211534
639.226091	-3.851268	72.216538
638.746676	-11.208302	72.221543
638.561020	0.462264	72.226548
638.031578	-8.856374	72.231553
637.260982	-0.870948	72.236558
636.276627	-8.440878	72.241562
635.903158	0.201957	72.246567
634.857783	6.105462	72.251572
633.995955	-4.409164	72.256577
633.195330	5.910155	72.261582
633.055302	-8.340017	72.266586
632.733266	1.382700	72.271591
631.801148	-8.759613	72.276596
631.292626	-4.065947	72.281601
630.392917	3.355008	72.286606
630.103149	1.223635	72.291610
629.370774	1.972814	72.296615
628.269881	0.735420	72.301620
627.848762	-2.319608	72.306625
627.213700	5.283125	72.311630
626.372426	-7.909219	72.316634
625.402415	-1.300219	72.321639
624.810489	11.314975	72.326644
624.765107	-1.920547	72.331649
623.776748	6.588410	72.336654
623.308287	-0.002411	72.341658
622.570942	-0.307396	72.346663
622.032795	7.363482	72.351668
621.335060	2.592667	72.356673
620.181802	12.916114	72.361678
620.054706	-2.394233	72.366682
619.471187	-2.482446	72.371687
618.403680	2.590399	72.376692
618.039951	-2.214682	72.381697
617.148175	-5.447058	72.386702
616.827621	-4.083810	72.391706
615.725107	5.930361	72.396711
614.702115	-0.863874	72.401716
614.436449	0.031751	72.406721
613.796291	-7.996676	72.411726
613.613268	-2.731963	72.416730
612.682204	-1.927482	72.421735
611.859588	-3.759531	72.426740
611.592115	-1.352933	72.431745
610.750130	-2.212092	72.436750
609.884768	2.738678	72.441754
609.382352	-5.396838	72.446759
609.053002	-6.720830	72.451764
608.044466	0.447809	72.456769
606.914485	4.057768	72.461774
606.483920	-11.732502	72.466778
606.049163	2.276879	72.471783
605.144619	-6.168321	72.476788
604.507837	-14.307662	72.481793
603.924011	5.916432	72.486798
603.659663	-6.259212	72.491802
602.927936	-0.104461	72.496807
601.740650	1.548212	72.501812
601.540145	-1.228140	72.506817
600.716356	7.459614	72.511822
600.258745	-1.873610	72.516826
599.362272	2.191160	72.521831
598.562049	-7.533761	72.526836
598.320495	-13.507865	72.531841
597.339557	1.326499	72.536846
596.691414	6.755177	72.541850
596.022166	-1.489382	72.546855
595.404968	-14.556547	72.551860
595.022526	-3.253605	72.556865
593.736390	5.141941	72.561870
593.272449	2.968928	72.566874
592.565577	7.333080	72.571879
592.295355	-0.842568	72.576884
591.639652	-11.068307	72.581889
590.767788	3.918996	72.586894
590.404256	0.164114	72.591898
589.596242	13.430303	72.596903
588.433273	-0.604906	72.601908
588.170325	4.887000	72.606913
587.409760	4.275072	72.611918
587.147997	-0.661360	72.616922
586.494182	-3.838586	72.621927
585.697098	0.306551	72.626932
585.034905	4.900126	72.631937
583.445477	13.981060	72.636942
582.987970	-11.458797	72.641946
582.529618	5.101063	72.646951
582.312514	-9.496358	72.651956
582.205443	-4.500780	72.656961
580.748020	2.036060	72.661966
580.267589	-5.929489	72.666970
579.658977	-2.282714	72.671975
579.359797	1.377855	72.676980
578.507368	-5.558640	72.681985
577.271785	11.610709	72.686990
577.463725	-2.141987	72.691994
576.428335	-2.044681	72.696999
575.064969	-2.210519	72.702004
574.779165	-0.294573	72.707009
574.065645	-1.748178	72.712014
574.122081	-1.430542	72.717018
573.148333	7.710023	72.722023
572.543249	6.060955	72.727028
572.163441	-3.801881	72.732033
570.711685	1.713797	72.737038
570.099257	-9.764591	72.742042
569.877927	5.514908	72.747047
568.690658	5.116026	72.752052
568.305374	1.099690	72.757057
567.486560	1.321773	72.762062
566.807801	0.307323	72.767066
566.549084	-1.780102	72.772071
565.761650	-7.142144	72.777076
565.115838	1.154576	72.782081
564.191823	-6.976851	72.787086
564.145256	-3.575710	72.792090
563.154120	-8.690843	72.797095
562.163827	-0.268294	72.802100
561.613832	-2.656245	72.807105
561.278398	-10.621227	72.812110
560.788732	-3.254529	72.817114
559.598555	-6.524506	72.822119
559.104700	-5.136802	72.827124
558.574120	-1.147645	72.832129
557.735112	-6.014202	72.837134
556.999287	-0.672476	72.842138
556.624004	-3.755289	72.847143
555.816233	-1.652125	72.852148
554.907648	-5.925716	72.857153
554.201883	-2.932073	72.862158
553.773551	1.594296	72.867162
553.227927	-2.429611	72.872167
552.606431	1.187684	72.877172
551.938802	0.693425	72.882177
551.305261	4.066641	72.887182
550.705614	-3.203414	72.892186
549.711352	-3.431185	72.897191
548.590674	-5.772385	72.902196
548.632882	-6.116365	72.907201
547.885753	0.390928	72.912206
547.557152	-3.071472	72.917210
546.565660	3.640322	72.922215
545.969752	3.073141	72.927220
545.450815	-1.866473	72.932225
544.283447	-4.952422	72.937230
543.704503	-4.071543	72.942234
543.030984	-1.740607	72.947239
542.778642	2.617385	72.952244
542.306494	0.813112	72.957249
541.292225	3.857478	72.962254
540.671918	-0.409991	72.967258
540.141954	-7.112413	72.972263
538.922869	-3.308465	72.977268
538.426181	-17.247912	72.982273
537.780921	0.278401	72.987278
537.356709	-1.358469	72.992282
537.346594	-12.470749	72.997287
536.065498	0.224261	73.002292
535.920794	-6.777642	73.007297
534.608325	-3.264739	73.012302
533.725089	2.374859	73.017306
533.444597	-2.389850	73.022311
532.621065	4.069696	73.027316
532.038214	-6.320589	73.032321
530.928617	-1.791351	73.037326
530.466486	5.957313	73.042330
530.186134	5.923328	73.047335
529.447698	6.815424	73.052340
528.694874	-6.253772	73.057345
527.785622	1.862574	73.062350
527.342436	-6.744389	73.067354
527.041716	-10.439877	73.072359
525.873467	-0.847284	73.077364
525.641180	-0.926771	73.082369
525.107770	-3.550739	73.087374
524.071510	-5.220993	73.092378
523.274430	-10.387520	73.097383
522.495761	-6.442416	73.102388
522.100194	-4.542095	73.107393
521.779930	-0.807203	73.112398
520.750318	-7.579834	73.117402
520.228478	-5.503284	73.122407
519.629630	-10.072198	73.127412
518.959829	-13.191663	73.132417
517.962178	0.705540	73.137422
517.526053	-11.149410	73.142426
517.214457	-2.032314	73.147431
515.879581	-4.989066	73.152436
515.226949	-6.961695	73.157441
514.567901	-2.909490	73.162446
514.323527	-9.308900	73.167450
513.648458	2.993121	73.172455
512.490007	-5.783741	73.177460
512.179508	-4.477275	73.182465
511.747942	0.219921	73.187470
511.178620	-5.865957	73.192474
510.390319	-4.486531	73.197479
509.356971	-2.997107	73.202484
508.865779	-5.362874	73.207489
508.404424	-1.141891	73.212494
507.486552	-10.586262	73.217498
506.704184	4.035148	73.222503
506.154578	-4.761433	73.227508
506.034446	-5.782856	73.232513
504.853959	7.831255	73.237518
504.358642	3.108656	73.242522
504.064811	3.851087	73.247527
502.810366	3.772013	73.252532
502.213202	-1.995623	73.257537
501.213884	-0.182041	73.262542
500.904156	-1.237914	73.267546
500.821881	-2.888249	73.272551
499.604646	2.353569	73.277556
498.975088	0.066615	73.282561
498.313616	10.377989	73.287566
497.800291	0.918053	73.292570
496.471073	10.645115	73.297575
496.213850	-3.362440	73.302580
496.059036	2.556932	73.307585
495.355191	1.877651	73.312590
494.655422	1.192990	73.317594
494.012195	-2.542546	73.322599
493.004347	9.821959	73.327604
492.354260	-2.002059	73.332609
491.609931	-2.963465	73.337614
491.133907	10.011736	73.342618
490.703268	-8.787239	73.347623
489.500379	-0.483760	73.352628
489.003514	9.555393	73.357633
488.461615	-0.942327	73.362638
487.763063	10.147644	73.367642
487.041418	-7.882744	73.372647
486.128087	3.142093	73.377652
486.017223	-0.796521	73.382657
485.186911	-5.815819	73.387662
484.397475	-2.483984	73.392666
484.176653	-6.263156	73.397671
483.177131	4.694991	73.402676
482.584633	6.785960	73.407681
481.224941	3.735411	73.412686
480.731455	-4.861950	73.417690
480.313313	6.773112	73.422695
480.002204	4.184700	73.427700
479.467214	-4.396587	73.432705
478.601045	7.987926	73.437710
478.064773	-3.575103	73.442714
477.428386	-1.524449	73.447719
476.270742	-3.648419	73.452724
476.014212	-2.618622	73.457729
475.361292	4.770945	73.462734
474.737891	-1.741537	73.467738
473.753360	-9.692973	73.472743
472.982922	-12.851583	73.477748
472.998992	-18.010444	73.482753
472.049060	-8.094659	73.487758
470.919723	-14.819835	73.492762
470.402716	-11.141903	73.497767
469.849282	-5.280450	73.502772
469.538244	-12.870837	73.507777
468.113058	-4.013132	73.512782
467.522325	-6.960681	73.517786
467.348531	-4.286728	73.522791
466.904054	-6.929580	73.527796
466.240440	-2.996482	73.532801
465.157830	-8.945377	73.537806
464.646403	-1.362317	73.542810
464.492534	-6.681760	73.547815
462.968190	-0.362851	73.552820
462.764495	-12.779926	73.557825
462.230287	3.446673	73.562830
461.517652	-2.133823	73.567834
460.323024	-10.879659	73.572839
459.716258	0.656144	73.577844
459.235671	2.221522	73.582849
459.045222	-11.763539	73.587854
458.010702	-5.432785	73.592858
457.017547	-8.757751	73.597863
456.404906	-3.090284	73.602868
456.283247	-11.589182	73.607873
455.917126	3.927835	73.612878
454.937298	-4.774955	73.617882
454.548515	-5.453959	73.622887
453.099490	-10.775203	73.627892
452.450622	-13.054335	73.632897
452.029466	-2.885328	73.637902
451.375193	-10.526680	73.642906
451.153340	-6.496810	73.647911
450.047394	5.842333	73.652916
449.582432	-6.351773	73.657921
449.092335	-3.879731	73.662926
448.140086	-1.291479	73.667930
447.395893	-5.780447	73.672935
446.503732	-4.236224	73.677940
446.393335	-7.599333	73.682945
445.203183	-3.199150	73.687950
444.596865	-4.565719	73.692954
443.936183	-8.602802	73.697959
443.562673	-7.723094	73.702964
443.266607	-9.555399	73.707969
442.133488	-0.318447	73.712974
441.604170	-1.238403	73.717978
440.985168	-1.849186	73.722983
440.235655	-0.682494	73.727988
439.607907	-11.448779	73.732993
438.636847	1.256793	73.737998
438.317376	-9.465573	73.743002
437.969696	-10.723543	73.748007
436.767625	-0.475840	73.753012
436.334357	-10.088850	73.758017
435.662635	0.198929	73.763022
434.629562	0.914075	73.768026
433.859411	-3.569176	73.773031
433.051429	-3.722504	73.778036
432.992646	-11.323115	73.783041
432.321511	-1.899578	73.788046
432.318497	-1.564589	73.793050
431.189615	-10.932726	73.798055
430.606156	1.228555	73.803060
429.453783	-4.567285	73.808065
428.645846	5.111436	73.813070
428.135353	0.399161	73.818074
427.996376	-6.468026	73.823079
427.034444	-5.000986	73.828084
426.085268	-10.526431	73.833089
425.351127	-4.178873	73.838094
424.821726	-4.871736	73.843098
424.570219	2.253612	73.848103
423.804115	1.585849	73.853108
422.945459	-4.263096	73.858113
422.443671	1.282641	73.863118
422.080952	-3.005335	73.868122
421.063118	-1.805345	73.873127
420.288785	3.864242	73.878132
420.035491	-4.774526	73.883137
419.210728	4.605688	73.888142
417.909078	-5.307336	73.893146
417.555901	-11.711468	73.898151
416.929633	-2.375500	73.903156
416.864337	-6.256714	73.908161
415.624988	5.305778	73.913166
415.235319	-7.412810	73.918170
414.597588	-5.336697	73.923175
413.879303	-9.363014	73.928180
412.953634	-9.697851	73.933185
412.564851	-6.494490	73.938190
412.022143	1.960865	73.943194
411.241753	-1.596677	73.948199
410.154315	6.609596	73.953204
410.138758	-9.784462	73.958209
409.487639	0.290309	73.963214
408.607222	0.443414	73.968218
407.668159	-7.882656	73.973223
407.108346	1.874800	73.978228
406.813188	-11.065417	73.983233
405.612781	5.708876	73.988238
404.688930	0.242477	73.993242
404.643614	-5.561022	73.998247
403.992570	3.206479	74.003252
403.809443	-10.656737	74.008257
402.710771	-1.355876	74.013262
401.960833	0.780696	74.018266
400.992863	-3.104910	74.023271
400.000920	5.931374	74.028276
399.729542	-15.907992	74.033281
399.153809	-0.460080	74.038286
398.557943	-3.789983	74.043290
398.177288	-10.374232	74.048295
397.205588	-7.333443	74.053300
396.722520	-2.899257	74.058305
396.126395	-3.355983	74.063310
395.190121	-5.915722	74.068314
394.620698	1.231900	74.073319
393.941166	10.114331	74.078324
393.599276	-8.364444	74.083329
392.447817	-5.201971	74.088334
391.708026	-1.102180	74.093338
391.378491	-9.954289	74.098343
390.752741	-2.450771	74.103348
390.392037	-10.891069	74.108353
389.274589	-8.703816	74.113358
388.837483	0.057979	74.118362
388.067478	-11.636496	74.123367
387.067872	5.460609	74.128372
386.535658	-14.146858	74.133377
385.816305	-2.772876	74.138382
385.581355	-10.766446	74.143386
384.960334	-7.921879	74.148391
383.618844	-8.706093	74.153396
383.047931	-7.848535	74.158401
382.751249	-11.005339	74.163406
382.437214	-2.652654	74.168410
381.548203	-15.078770	74.173415
380.682124	-5.570547	74.178420
380.252605	-10.724630	74.183425
379.698888	-6.334376	74.188430
378.823487	-15.946294	74.193434
378.481944	-10.251054	74.198439
377.673108	-7.368672	74.203444
376.424300	-10.490442	74.208449
375.957845	-13.866189	74.213454
375.336563	-1.935414	74.218458
375.037501	-10.082764	74.223463
373.763259	-15.283578	74.228468
373.410194	-6.893136	74.233473
372.789104	-5.090894	74.238478
372.424255	-3.480869	74.243482
371.640742	-13.041198	74.248487
370.656495	-4.247405	74.253492
370.380663	-14.314401	74.258497
369.994924	-10.608487	74.263502
368.712925	-2.751236	74.268506
368.280574	-7.252024	74.273511
367.576958	8.760313	74.278516
367.342262	-20.510563	74.283521
365.892912	1.970824	74.288526
365.390111	-11.565480	74.293530
365.117315	-11.433497	74.298535
364.095987	-6.743224	74.303540
363.542858	-12.995634	74.308545
362.775195	-0.913800	74.313550
362.179866	-7.273025	74.318554
362.116439	-16.407220	74.323559
360.824253	0.840587	74.328564
360.444519	-19.291042	74.333569
359.687922	-1.776939	74.338574
358.903535	-11.128972	74.343578
358.268405	-7.659272	74.348583
357.383524	-7.618974	74.353588
356.989179	-4.365836	74.358593
356.660800	-2.518776	74.363598
355.690971	-3.086244	74.368602
355.177604	-4.249989	74.373607
354.309622	3.473485	74.378612
353.632138	-8.912217	74.383617
352.565803	2.518648	74.388622
352.114221	-1.092850	74.393626
351.884159	-5.315221	74.398631
351.150139	0.234419	74.403636
350.455190	-16.456615	74.408641
349.575560	-7.050302	74.413646
349.125597	-10.636824	74.418650
348.613740	-9.121636	74.423655
347.658578	-4.727322	74.428660
347.094593	-1.816144	74.433665
346.489788	-18.343349	74.438670
345.874438	4.512902	74.443674
344.895985	-13.660979	74.448679
344.026575	-2.439690	74.453684
343.921620	-15.146855	74.458689
343.235159	-13.849838	74.463694
342.475468	-3.817680	74.468698
341.865502	-16.187324	74.473703
340.917412	-5.191610	74.478708
340.682757	-14.740051	74.483713
339.684285	-6.216788	74.488718
338.858317	-5.345379	74.493722
338.725936	-22.059827	74.498727
337.925213	-2.777282	74.503732
337.337684	-15.856957	74.508737
336.462003	1.244058	74.513742
335.843606	-10.624363	74.518746
335.424110	-2.418867	74.523751
334.410248	-6.232477	74.528756
333.671079	-8.744758	74.533761
333.254935	-8.071123	74.538766
332.764194	-10.132577	74.543770
331.676105	-13.518049	74.548775
330.813926	-15.588112	74.553780
330.561236	-8.866268	74.558785
330.250091	-15.791151	74.563790
329.276217	-1.317390	74.568794
328.909468	-11.425081	74.573799
328.384299	-10.557455	74.578804
327.203763	-9.281037	74.583809
326.317589	-5.736627	74.588814
325.724645	-3.144096	74.593818
325.998711	-2.692422	74.598823
324.227931	-6.035319	74.603828
323.963821	-4.157499	74.608833
323.344072	-0.343320	74.613838
322.777379	-12.875970	74.618842
321.613936	-6.636582	74.623847
320.699822	-3.802057	74.628852
320.604465	-6.391713	74.633857
320.273371	-8.915413	74.638862
319.810827	-8.064074	74.643866
318.795565	-4.648894	74.648871
317.891954	-9.079293	74.653876
317.726745	-5.572518	74.658881
316.488874	-7.171126	74.663886
315.658932	-2.522375	74.668890
315.592019	-10.031794	74.673895
314.753518	-2.257819	74.678900
314.286979	-7.637793	74.683905
313.024622	-4.102807	74.688910
312.703530	-10.669721	74.693914
312.119380	-10.227919	74.698919
311.291108	1.783164	74.703924
310.869293	1.304985	74.708929
309.992827	-12.155974	74.713934
309.716652	-15.352303	74.718938
308.948057	-6.315328	74.723943
307.902643	1.045364	74.728948
307.224588	-22.425899	74.733953
306.854744	-19.130932	74.738958
306.064901	-1.269334	74.743962
305.547160	-4.132281	74.748967
304.616610	-5.778288	74.753972
304.323244	-9.996870	74.758977
303.453270	-3.678095	74.763982
302.415930	-8.486132	74.768986
302.278990	-13.306793	74.773991
301.972786	-5.453657	74.778996
301.292055	-8.815736	74.784001
300.127291	-11.370556	74.789006
299.228634	-5.876664	74.794010
299.157617	-10.846601	74.799015
298.004296	-9.781082	74.804020
297.543427	-10.118996	74.809025
296.888856	-16.147064	74.814030
296.206480	-9.590116	74.819034
295.459047	-10.339659	74.824039
294.502522	-11.918445	74.829044
294.087855	2.709043	74.834049
293.811215	-9.579679	74.839054
293.135749	-8.543014	74.844058
292.471395	-13.259111	74.849063
291.241713	-9.670978	74.854068
291.241840	-14.087719	74.859073
290.028844	-12.374036	74.864078
289.293003	-4.778841	74.869082
288.909625	-4.294919	74.874087
288.330113	1.589646	74.879092
288.215539	-8.780575	74.884097
286.983331	-1.304952	74.889102
286.190616	-10.925279	74.894106
286.014805	-10.993245	74.899111
284.556679	-2.196430	74.904116
284.040383	0.265625	74.909121
283.695893	-5.211065	74.914126
283.240628	2.038224	74.919130
282.578687	-1.333153	74.924135
281.002372	5.629637	74.929140
280.929035	-5.658613	74.934145
280.371651	8.606862	74.939150
279.821718	-6.878850	74.944154
278.785606	3.970072	74.949159
278.227273	-1.240727	74.954164
277.685917	2.297623	74.959169
277.080283	-0.174427	74.964174
276.471858	-4.568285	74.969178
275.904524	-1.049448	74.974183
275.074116	2.225901	74.979188
274.897780	-6.871369	74.984193
273.548938	3.940672	74.989198
272.883483	-2.650193	74.994202
272.626844	-8.244959	74.999207
272.141477	5.280502	75.004212
271.359058	-6.262140	75.009217
270.540098	-3.054846	75.014222
269.866428	-0.867316	75.019226
269.094934	-8.016848	75.024231
268.079595	2.256347	75.029236
267.698981	-11.201631	75.034241
267.379964	-4.740439	75.039246
266.635832	-5.320193	75.044250
265.714550	-9.514371	75.049255
265.192473	0.587160	75.054260
264.885037	-5.565619	75.059265
263.779299	-7.213646	75.064270
263.110595	5.964159	75.069274
262.638369	7.017320	75.074279
261.981770	3.093178	75.079284
260.932368	-3.868555	75.084289
260.244308	-9.345665	75.089294
259.551773	7.965867	75.094298
259.663785	-3.500155	75.099303
258.708363	-1.434864	75.104308
257.893049	-6.095350	75.109313
257.081951	-10.982005	75.114318
256.573557	-4.329780	75.119322
256.379782	-4.196190	75.124327
255.208361	-4.681021	75.129332
254.518354	1.452968	75.134337
254.224882	0.027117	75.139342
253.163104	-1.627912	75.144346
252.393604	-0.573093	75.149351
251.646108	6.533555	75.154356
251.493675	1.884093	75.159361
250.747830	4.034249	75.164366
249.856415	2.755752	75.169370
249.282725	-2.384783	75.174375
248.457957	2.444509	75.179380
248.140415	-1.875865	75.184385
247.116530	-4.256003	75.189390
246.084407	-1.528794	75.194394
246.300970	0.879521	75.199399
245.405925	-2.238649	75.204404
245.283933	2.382425	75.209409
244.306899	4.121593	75.214414
243.745433	6.341705	75.219418
242.671365	-2.409035	75.224423
241.808403	9.894596	75.229428
241.668667	-2.900053	75.234433
241.081022	-1.609300	75.239438
239.954498	2.694102	75.244442
239.659535	-1.346026	75.249447
238.684208	1.561363	75.254452
237.756488	4.956313	75.259457
236.935420	-8.018294	75.264462
236.483139	-3.816067	75.269466
236.367288	0.127532	75.274471
235.437277	4.555724	75.279476
235.090864	-5.195653	75.284481
234.210358	-0.693355	75.289486
233.481999	0.954138	75.294490
232.980194	-5.932452	75.299495
231.871456	13.369266	75.304500
231.024609	3.822236	75.309505
230.898321	6.359320	75.314510
230.366678	7.779918	75.319514
229.781545	-8.196889	75.324519
228.670861	-4.365928	75.329524
228.211831	8.873073	75.334529
227.505684	5.218607	75.339534
226.916032	-2.660047	75.344538
226.237320	-2.341918	75.349543
225.289386	-3.873161	75.354548
225.268935	0.741185	75.359553
224.193840	-1.302782	75.364558
223.035241	-4.785770	75.369562
222.710823	-5.976454	75.374567
222.388212	-0.060295	75.379572
222.148293	-4.996994	75.384577
220.979746	-6.914101	75.389582
220.261188	4.603286	75.394586
220.049706	-10.190475	75.399591
218.798797	4.428404	75.404596
218.053471	-8.692305	75.409601
217.578342	-6.687798	75.414606
217.035011	-8.395499	75.419610
216.173890	-2.320954	75.424615
215.151929	-4.780230	75.429620
214.573231	4.049885	75.434625
214.455130	-2.104686	75.439630
213.940361	-1.541461	75.444634
213.466280	-12.177621	75.449639
212.230832	-2.433856	75.454644
211.827316	-5.548373	75.459649
210.727532	-5.700837	75.464654
209.778078	1.392284	75.469658
209.742235	-8.810708	75.474663
209.136056	4.781323	75.479668
208.907189	1.591656	75.484673
207.930384	-5.220778	75.489678
206.752482	4.764548	75.494682
206.600349	-8.871760	75.499687
205.504535	-0.208357	75.504692
204.939783	1.088217	75.509697
204.374725	-3.299919	75.514702
203.763178	1.238357	75.519706
203.431350	-8.338722	75.524711
202.279335	-5.526152	75.529716
201.526558	-2.293119	75.534721
201.441480	-0.639367	75.539726
200.388519	4.674161	75.544730
199.817748	-4.560481	75.549735
199.041492	-0.180445	75.554740
198.938360	-1.926784	75.559745
197.686572	9.404393	75.564750
197.196254	3.775929	75.569754
196.854545	-0.646236	75.574759
195.884191	2.586796	75.579764
194.812091	-2.401726	75.584769
194.356721	-8.065717	75.589774
193.858537	-1.757300	75.594778
193.666596	-5.493731	75.599783
192.302242	6.697462	75.604788
191.952457	-2.692256	75.609793
191.291827	6.177733	75.614798
190.470892	6.977427	75.619802
189.921225	-2.183310	75.624807
188.899789	9.633103	75.629812
188.509031	0.828642	75.634817
188.167576	8.357835	75.639822
187.032050	3.611234	75.644826
186.639601	7.218898	75.649831
185.872958	-0.388681	75.654836
185.138617	7.035998	75.659841
184.275557	2.829414	75.664846
183.541571	-1.340977	75.669850
183.256536	0.682114	75.674855
182.566251	2.883353	75.679860
182.393367	3.511922	75.684865
181.518020	3.189651	75.689870
180.657226	-0.722409	75.694874
180.526787	-7.816421	75.699879
179.166630	8.060921	75.704884
178.613187	-6.377123	75.709889
178.168830	5.801432	75.714894
177.113273	-4.352518	75.719898
176.211059	-0.816539	75.724903
175.738698	-5.238368	75.729908
175.422159	-13.269350	75.734913
175.230579	-2.750587	75.739918
174.157747	-0.225010	75.744922
173.685094	-5.424208	75.749927
172.843955	-0.907667	75.754932
171.867158	-4.865880	75.759937
170.998872	-2.249916	75.764942
170.123408	-10.891932	75.769946
170.026902	-7.881794	75.774951
169.271959	7.522176	75.779956
169.211983	-2.995503	75.784961
168.196865	-5.430619	75.789966
167.555832	-3.934223	75.794970
167.024900	-6.894378	75.799975
165.811585	4.410174	75.804980
165.138806	-1.324802	75.809985
164.902306	-2.671417	75.814990
164.216832	-0.234405	75.819994
163.324135	-3.603644	75.824999
162.517561	8.908626	75.830004
162.224332	-9.793861	75.835009
161.902297	-6.987454	75.840014
160.663138	1.727205	75.845018
160.090592	-14.393494	75.850023
159.286827	4.962104	75.855028
158.721638	-7.539192	75.860033
158.440147	-7.114072	75.865038
157.514801	-5.233307	75.870042
157.421165	-5.328558	75.875047
156.378817	-3.265138	75.880052
155.147598	-6.501553	75.885057
154.590093	-8.479785	75.890062
154.039308	0.271771	75.895066
154.157888	-4.051892	75.900071
152.947242	8.305616	75.905076
152.201603	-6.229503	75.910081
151.759734	-1.377661	75.915086
150.752848	2.365822	75.920090
149.508739	-10.777824	75.925095
149.112951	-3.172164	75.930100
148.652962	-1.594247	75.935105
148.367801	1.963199	75.940110
148.231931	3.148825	75.945114
147.464031	-5.901407	75.950119
146.381707	-8.328950	75.955124
146.122950	1.962413	75.960129
144.739495	-12.735918	75.965134
143.935828	6.611783	75.970138
143.910824	-5.223455	75.975143
143.115356	-1.980445	75.980148
141.944954	-8.634247	75.985153
141.396683	2.537464	75.990158
140.832471	8.350233	75.995162
140.540458	-1.048685	76.000167
139.929116	-3.754746	76.005172
139.189379	-7.443246	76.010177
138.586120	-11.317505	76.015182
137.563554	1.579278	76.020186
136.744805	-11.493416	76.025191
135.775000	5.102266	76.030196
135.398308	-11.243616	76.035201
134.947759	-0.533753	76.040206
134.958171	-0.852169	76.045210
134.260855	-2.369722	76.050215
133.221179	-8.995480	76.055220
132.595382	4.104537	76.060225
131.625796	-9.097065	76.065230
130.504607	-2.854875	76.070234
130.325541	-9.971086	76.075239
130.101920	-12.291124	76.080244
129.426672	-10.317768	76.085249
128.402170	-6.677123	76.090254
127.738166	-8.199986	76.095258
127.297389	-15.944648	76.100263
125.766386	-5.978686	76.105268
125.504535	-8.153861	76.110273
125.264410	-1.440319	76.115278
124.729391	-1.637070	76.120282
124.237314	-2.955542	76.125287
123.228855	-8.805703	76.130292
122.889066	-8.465898	76.135297
122.103820	-3.305416	76.140302
120.847893	-9.193384	76.145306
120.436353	-10.791194	76.150311
119.861474	-2.204522	76.155316
119.549108	-8.973056	76.160321
118.191298	-16.607755	76.165326
117.593175	-1.067950	76.170330
117.379990	-15.478219	76.175335
116.640524	-2.172429	76.180340
116.247740	-6.346742	76.185345
115.529589	-11.801657	76.190350
114.892202	0.541715	76.195354
113.636415	-11.601862	76.200359
112.528602	-0.806113	76.205364
112.010749	-6.031202	76.210369
112.124657	-13.168897	76.215374
111.659891	-9.075046	76.220378
111.032843	-0.073211	76.225383
110.032548	-2.157438	76.230388
109.667401	-2.685617	76.235393
108.397782	-2.402534	76.240398
107.425156	-7.036299	76.245402
107.072833	-3.625832	76.250407
106.788859	-2.959043	76.255412
106.266077	-8.058769	76.260417
105.184786	9.363656	76.265422
104.340931	-2.243233	76.270426
104.347337	-0.183033	76.275431
103.712151	-0.928339	76.280436
102.786609	-4.314393	76.285441
101.930226	-5.521151	76.290446
101.396346	9.910655	76.295450
101.096522	-10.875432	76.300455
99.646690	-0.499786	76.305460
99.319165	-11.272819	76.310465
99.214614	0.316976	76.315470
97.434875	-0.821380	76.320474
96.953007	-2.701276	76.325479
96.438057	7.438563	76.330484
96.330278	3.023265	76.335489
95.949055	-5.052581	76.340494
95.048468	5.464135	76.345498
94.462225	6.849314	76.350503
93.472038	0.706098	76.355508
92.567839	-5.406674	76.360513
91.688944	3.010873	76.365518
91.284339	-1.577855	76.370522
91.056906	-2.936946	76.375527
90.525282	-1.920012	76.380532
89.539275	-5.747414	76.385537
88.925025	-12.289608	76.390542
87.980143	-0.966339	76.395546
87.589372	-17.893407	76.400551
86.624564	-8.323639	76.405556
86.032890	-15.862882	76.410561
85.784780	-9.234799	76.415566
84.814762	-6.503239	76.420570
83.970080	-9.280878	76.425575
83.063174	-9.962346	76.430580
82.692821	3.656742	76.435585
82.318410	-7.304350	76.440590
81.525982	7.875382	76.445594
81.046320	-12.008409	76.450599
80.341996	2.442928	76.455604
79.638955	-8.397946	76.460609
78.952419	-6.137357	76.465614
77.919997	-7.109457	76.470618
77.820979	-7.566534	76.475623
77.073313	-6.086226	76.480628
76.445135	-1.269315	76.485633
75.506564	0.627781	76.490638
74.720634	3.564948	76.495642
74.684767	-12.679151	76.500647
73.722875	-2.468040	76.505652
73.006940	7.509895	76.510657
72.505144	-2.140972	76.515662
71.509260	-0.630537	76.520666
70.788668	-8.158681	76.525671
70.246097	-1.493095	76.530676
70.163749	1.070099	76.535681
69.165089	-4.247029	76.540686
68.414096	-9.941111	76.545690
67.905143	-8.721214	76.550695
66.824766	-8.187600	76.555700
66.108794	-5.469741	76.560705
65.698270	-4.658191	76.565710
64.761422	7.034382	76.570714
65.043627	-9.348752	76.575719
63.519883	10.377145	76.580724
63.013338	3.060860	76.585729
62.556720	-1.242032	76.590734
61.952584	-4.480637	76.595738
60.936864	-1.060555	76.600743
60.045905	-7.227461	76.605748
59.490685	5.151702	76.610753
59.224790	-2.983529	76.615758
58.363504	3.669815	76.620762
57.797942	-5.139845	76.625767
56.996934	2.368029	76.630772
56.929343	7.164926	76.635777
55.900520	-2.684149	76.640782
54.803054	-0.687589	76.645786
54.508674	-4.975352	76.650791
54.153640	-9.532553	76.655796
52.810517	-2.751903	76.660801
52.638153	-11.255272	76.665806
51.938159	5.466126	76.670810
51.392715	-12.891752	76.675815
50.189549	3.075709	76.680820
49.371176	-3.588458	76.685825
48.873886	-2.723644	76.690830
48.710670	4.414440	76.695834
48.409244	-2.693286	76.700839
47.233853	-0.504527	76.705844
46.463480	-6.135589	76.710849
46.223918	-4.974421	76.715854
45.070811	-2.112723	76.720858
44.268024	8.208642	76.725863
44.065730	-8.996055	76.730868
43.492701	7.120063	76.735873
42.359534	-4.218307	76.740878
41.466921	8.287208	76.745882
41.280195	-5.464972	76.750887
40.860744	7.761416	76.755892
40.239962	-5.738614	76.760897
39.522272	-6.343014	76.765902
38.348971	1.400855	76.770906
38.584644	-14.604277	76.775911
37.225997	3.650846	76.780916
36.655912	-9.224925	76.785921
36.373141	-2.777384	76.790926
34.749952	3.470797	76.795930
34.427259	-11.913864	76.800935
33.850830	-13.930046	76.805940
33.318557	-6.663722	76.810945
33.150502	-8.137929	76.815950
32.200327	1.979868	76.820954
31.822368	-10.754660	76.825959
30.736943	-14.408485	76.830964
29.605809	-1.628397	76.835969
29.117732	-9.693488	76.840974
28.922457	-14.151588	76.845978
28.326753	-6.584996	76.850983
27.332803	-11.180630	76.855988
26.414488	-7.496960	76.860993
26.296879	-5.528943	76.865998
25.547217	-5.492747	76.871002
24.743057	-3.968721	76.876007
23.901634	-0.038699	76.881012
23.572114	-9.953559	76.886017
22.882780	-3.009100	76.891022
21.630638	-7.046327	76.896026
21.333983	-2.857853	76.901031
20.653707	3.894359	76.906036
20.138500	-13.386570	76.911041
19.727725	-2.146897	76.916046
18.288197	1.345530	76.921050
18.256836	-8.180083	76.926055
17.553408	-1.954020	76.931060
16.972615	-8.301262	76.936065
16.436070	-4.287408	76.941070
15.468336	-7.925307	76.946074
15.226190	-2.763115	76.951079
13.856868	-8.513089	76.956084
13.616999	-8.025209	76.961089
13.030119	-5.122928	76.966094
12.269556	0.487796	76.971098
11.595732	-13.520980	76.976103
10.524055	0.332966	76.981108
9.909609	-1.661378	76.986113
9.905103	-5.187994	76.991118
9.083980	3.754932	76.996122
8.362158	-7.529183	77.001127
7.580843	-10.976046	77.006132
6.837302	3.289175	77.011137
5.751825	-7.342440	77.016142
5.138830	-0.444844	77.021147
5.106246	-8.111088	77.026151
4.326878	-10.791885	77.031156
3.934483	-5.214656	77.036161