Mon Mar 08 18:11:25 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.623372	99.804041	0.000000
-0.676288	96.657230	0.005005
-1.353624	70.703833	0.010010
-2.764256	26.059714	0.015014
-5.843903	-19.365085	0.020019
-11.436752	-33.872739	0.025024
-16.857421	-35.084634	0.030029
-22.057708	-27.310245	0.035034
-25.807048	-37.114760	0.040038
-29.542520	-39.532141	0.045043
-33.271293	-31.065267	0.050048
-36.871800	-31.402165	0.055053
-40.725349	-32.441407	0.060058
-43.818523	-36.358365	0.065062
-47.936676	-33.903555	0.070067
-51.639538	-29.531257	0.075072
-55.543143	-28.944593	0.080077
-59.771611	-29.402037	0.085082
-63.047172	-44.734981	0.090086
-66.671695	-36.898107	0.095091
-70.469162	-36.889728	0.100096
-73.910718	-28.588463	0.105101
-78.013959	-28.879781	0.110106
-81.722592	-39.017114	0.115110
-85.781085	-34.330991	0.120115
-89.237622	-35.854531	0.125120
-92.954650	-36.467633	0.130125
-96.663735	-37.911443	0.135130
-100.607937	-38.808395	0.140134
-104.622923	-34.118145	0.145139
-108.405799	-39.818818	0.150144
-112.213226	-54.778238	0.155149
-116.111484	-37.461485	0.160154
-119.760527	-35.634898	0.165158
-123.694275	-21.866774	0.170163
-127.472758	-32.156888	0.175168
-130.998331	-37.813431	0.180173
-134.792599	-32.451904	0.185178
-138.127325	-37.465556	0.190182
-142.019906	-28.805233	0.195187
-145.853844	-37.676719	0.200192
-149.402217	-31.337311	0.205197
-153.634223	-31.631605	0.210202
-156.972800	-37.437794	0.215206
-160.991296	-34.609205	0.220211
-164.634512	-33.571929	0.225216
-168.109945	-38.859539	0.230221
-172.331706	-24.318433	0.235226
-175.852632	-42.530883	0.240230
-179.926544	-34.565361	0.245235
-183.654689	-38.935863	0.250240
-187.140577	-36.192233	0.255245
-191.230449	-35.391126	0.260250
-194.700697	-35.191934	0.265254
-198.658251	-33.424797	0.270259
-202.327874	-45.950839	0.275264
-206.039592	-22.739326	0.280269
-209.679035	-31.635443	0.285274
-213.624492	-43.825718	0.290278
-217.436575	-37.242285	0.295283
-221.027913	-41.304992	0.300288
-224.644464	-41.341015	0.305293
-228.509438	-31.357225	0.310298
-232.357354	-36.012874	0.315302
-236.335795	-36.405839	0.320307
-240.168169	-36.065205	0.325312
-243.601532	-30.933000	0.330317
-247.550672	-31.072014	0.335322
-250.707017	-40.904577	0.340326
-255.104569	-42.742851	0.345331
-258.761901	-43.276918	0.350336
-262.513525	-34.372421	0.355341
-266.627054	-28.437778	0.360346
-269.870882	-33.688094	0.365350
-273.923675	-33.643367	0.370355
-277.418384	-32.240136	0.375360
-281.128540	-26.529126	0.380365
-285.357902	-20.642188	0.385370
-289.069297	-37.215618	0.390374
-292.782776	-36.990070	0.395379
-296.335279	-30.563068	0.400384
-299.918865	-29.574530	0.405389
-303.813161	-24.445923	0.410394
-307.362282	-43.509904	0.415398
-311.325308	-33.136614	0.420403
-315.157302	-32.455312	0.425408
-318.922472	-32.401237	0.430413
-322.809279	-38.975911	0.435418
-326.397845	-31.778317	0.440422
-330.060645	-33.221270	0.445427
-334.108856	-23.785204	0.450432
-337.828066	-28.838107	0.455437
-341.838453	-23.676714	0.460442
-345.303090	-38.108601	0.465446
-349.062926	-28.880977	0.470451
-352.829591	-25.060992	0.475456
-356.244738	-38.100482	0.480461
-360.753896	-27.043849	0.485466
-363.889505	-35.930276	0.490470
-368.172641	-33.852268	0.495475
-371.319571	-32.657389	0.500480
-374.976787	-33.278027	0.505485
-379.390860	-42.855964	0.510490
-382.787235	-37.964433	0.515494
-386.985577	-18.935736	0.520499
-390.695102	-26.554127	0.525504
-393.982981	-38.685091	0.530509
-397.884281	-33.334457	0.535514
-401.484296	-32.560755	0.540518
-405.737348	-27.650658	0.545523
-409.333940	-21.937091	0.550528
-412.614026	-36.582837	0.555533
-417.016669	-37.037066	0.560538
-420.729761	-30.592128	0.565542
-424.347519	-28.893078	0.570547
-428.122645	-27.277697	0.575552
-431.255142	-38.386363	0.580557
-435.629527	-30.508055	0.585562
-439.198242	-42.512099	0.590566
-443.274819	-42.425442	0.595571
-446.850240	-51.288809	0.600576
-450.640257	-24.885475	0.605581
-454.596931	-26.033731	0.610586
-458.319268	-32.080956	0.615590
-461.992668	-36.245299	0.620595
-465.681052	-34.678404	0.625600
-469.075125	-35.941719	0.630605
-473.197742	-38.071070	0.635610
-476.932114	-44.641442	0.640614
-480.583426	-33.748421	0.645619
-484.703461	-31.888636	0.650624
-488.230290	-33.103913	0.655629
-492.210035	-29.345872	0.660634
-495.845931	-39.929356	0.665638
-499.823680	-38.836565	0.670643
-503.165202	-36.394652	0.675648
-506.784667	-39.597751	0.680653
-510.753751	-30.325428	0.685658
-514.641925	-39.490385	0.690662
-518.552948	-33.426831	0.695667
-521.951907	-37.395229	0.700672
-525.727171	-32.441401	0.705677
-529.981100	-24.861276	0.710682
-533.302178	-32.636093	0.715686
-536.841039	-33.157121	0.720691
-540.800468	-33.434349	0.725696
-544.617977	-39.448881	0.730701
-548.578990	-29.624301	0.735706
-552.348146	-40.071292	0.740710
-556.102310	-30.270283	0.745715
-559.570990	-32.240610	0.750720
-563.165589	-37.686774	0.755725
-567.442691	-35.902677	0.760730
-571.180819	-46.058133	0.765734
-574.966701	-33.818897	0.770739
-578.746034	-23.996483	0.775744
-582.275280	-29.845707	0.780749
-586.196612	-30.701356	0.785754
-589.550900	-40.948068	0.790758
-593.419072	-32.776638	0.795763
-597.404844	-28.375669	0.800768
-601.258275	-33.621156	0.805773
-604.980789	-30.485900	0.810778
-608.332228	-40.633696	0.815782
-612.511864	-35.121564	0.820787
-616.102084	-29.053919	0.825792
-619.988733	-36.886468	0.830797
-623.805319	-32.151382	0.835802
-627.219316	-39.639984	0.840806
-631.204265	-23.887087	0.845811
-634.620299	-37.763323	0.850816
-638.619489	-39.185160	0.855821
-642.637576	-32.558700	0.860826
-646.188163	-33.935516	0.865830
-649.941032	-30.470502	0.870835
-653.900033	-29.744710	0.875840
-657.673114	-31.964282	0.880845
-661.550530	-34.756931	0.885850
-664.896181	-42.861919	0.890854
-668.611189	-25.069037	0.895859
-672.561731	-28.949073	0.900864
-676.745343	-36.210544	0.905869
-680.119218	-35.149299	0.910874
-683.477356	-46.800252	0.915878
-687.486553	-29.512247	0.920883
-691.418655	-29.905549	0.925888
-695.253966	-37.526984	0.930893
-698.966566	-29.370789	0.935898
-702.634578	-42.197436	0.940902
-706.669074	-35.736978	0.945907
-710.040013	-33.033045	0.950912
-713.642932	-27.983473	0.955917
-717.757675	-25.189041	0.960922
-721.324867	-33.640150	0.965926
-725.356410	-25.869738	0.970931
-729.181784	-29.895832	0.975936
-732.689003	-33.487087	0.980941
-736.426065	-36.672609	0.985946
-740.217764	-37.491951	0.990950
-744.195900	-32.812856	0.995955
-747.962602	-35.747628	1.000960
-751.668660	-32.728312	1.005965
-755.792315	-32.874857	1.010970
-758.892962	-39.747897	1.015974
-762.843297	-42.121883	1.020979
-766.564034	-38.176146	1.025984
-769.859924	-36.909628	1.030989
-774.211976	-24.560673	1.035994
-777.905891	-30.231889	1.040998
-781.995318	-32.121585	1.046003
-785.371303	-29.724233	1.051008
-789.313573	-35.742066	1.056013
-793.522153	-32.284406	1.061018
-796.484553	-28.762601	1.066022
-800.011533	-34.977682	1.071027
-803.942631	-26.721750	1.076032
-807.840128	-37.463166	1.081037
-811.929828	-42.353571	1.086042
-815.548752	-30.629502	1.091046
-819.436074	-34.281281	1.096051
-823.292582	-36.851506	1.101056
-826.500156	-40.261869	1.106061
-830.417032	-36.447097	1.111066
-834.056168	-31.120335	1.116070
-837.851915	-32.353592	1.121075
-842.146952	-28.432613	1.126080
-845.664898	-39.081682	1.131085
-849.671609	-28.782567	1.136090
-852.913740	-41.032101	1.141094
-857.243698	-37.096052	1.146099
-860.884648	-20.532093	1.151104
-864.174068	-32.662098	1.156109
-868.206804	-29.612449	1.161114
-871.810106	-40.339287	1.166118
-875.601014	-31.326679	1.171123
-879.247213	-27.961938	1.176128
-882.901187	-32.169713	1.181133
-887.119881	-29.396215	1.186138
-890.716429	-33.680964	1.191142
-894.751053	-35.021007	1.196147
-898.517418	-29.225972	1.201152
-902.089757	-36.772411	1.206157
-905.809449	-37.953065	1.211162
-909.459185	-27.904890	1.216166
-913.288733	-33.010171	1.221171
-917.029464	-35.951974	1.226176
-920.513900	-41.771560	1.231181
-924.851590	-25.040916	1.236186
-928.178131	-39.345709	1.241190
-931.975652	-34.813453	1.246195
-935.682728	-48.893377	1.251200
-939.328127	-44.104754	1.256205
-943.457544	-37.204547	1.261210
-947.125194	-43.463126	1.266214
-951.211713	-43.881758	1.271219
-955.052031	-27.082377	1.276224
-958.439308	-42.001851	1.281229
-962.393533	-33.887047	1.286234
-966.036116	-37.066805	1.291238
-969.711517	-37.893335	1.296243
-973.305750	-33.573289	1.301248
-977.112123	-34.281095	1.306253
-981.241976	-27.276676	1.311258
-984.818860	-38.993103	1.316262
-988.650335	-45.006226	1.321267
-992.337272	-26.132495	1.326272
-995.943830	-31.399451	1.331277
-1000.138193	-19.535773	1.336282
-1003.448013	-36.651549	1.341286
-1007.213988	-32.606744	1.346291
-1011.273069	-28.989694	1.351296
-1014.794860	-37.597391	1.356301
-1018.901526	-24.861507	1.361306
-1022.261205	-27.808896	1.366310
-1026.050092	-27.174341	1.371315
-1029.992832	-30.801130	1.376320
-1033.758640	-29.455927	1.381325
-1037.707391	-26.040974	1.386330
-1040.970735	-29.235545	1.391334
-1044.367117	-34.140244	1.396339
-1048.581956	-28.993874	1.401344
-1052.524928	-33.628211	1.406349
-1056.902680	-15.064902	1.411354
-1060.352070	-19.379235	1.416358
-1063.901295	-28.165389	1.421363
-1067.181374	-37.849253	1.426368
-1070.693763	-43.700401	1.431373
-1075.312343	-24.604986	1.436378
-1079.088098	-28.039216	1.441382
-1082.562250	-36.523545	1.446387
-1086.446003	-33.065296	1.451392
-1089.948353	-33.824707	1.456397
-1093.807324	-26.169606	1.461402
-1097.611481	-34.422931	1.466406
-1101.008022	-31.881501	1.471411
-1105.132832	-33.637237	1.476416
-1108.762824	-41.076350	1.481421
-1113.314325	-35.056032	1.486426
-1116.732385	-33.346881	1.491430
-1120.163051	-31.873818	1.496435
-1123.672495	-35.057279	1.501440
-1127.529243	-30.409588	1.506445
-1131.599736	-29.147939	1.511450
-1135.096470	-29.192277	1.516454
-1138.957019	-34.073028	1.521459
-1143.046403	-27.964170	1.526464
-1146.569190	-37.944956	1.531469
-1150.564597	-36.326299	1.536474
-1153.912245	-39.964510	1.541478
-1157.550928	-23.561351	1.546483
-1161.605659	-34.959766	1.551488
-1164.918403	-39.924969	1.556493
-1169.281302	-34.259558	1.561498
-1172.938462	-43.936535	1.566502
-1176.548346	-37.475438	1.571507
-1180.379919	-33.208564	1.576512
-1183.680122	-41.816752	1.581517
-1188.041336	-26.758124	1.586522
-1191.688096	-37.974193	1.591526
-1195.546766	-43.039639	1.596531
-1199.371926	-34.219744	1.601536
-1202.694279	-46.213062	1.606541
-1206.845992	-31.295159	1.611546
-1210.630844	-28.284597	1.616550
-1214.206710	-42.517495	1.621555
-1217.698460	-45.378804	1.626560
-1221.357681	-50.987027	1.631565
-1226.063250	-31.521059	1.636570
-1229.679568	-44.599489	1.641574
-1232.838579	-36.502709	1.646579
-1236.377772	-34.789767	1.651584
-1240.458671	-37.903669	1.656589
-1244.239552	-40.573593	1.661594
-1248.160975	-46.581336	1.666598
-1252.241404	-30.364385	1.671603
-1256.104425	-33.278175	1.676608
-1259.447855	-41.428344	1.681613
-1262.799518	-38.182694	1.686618
-1266.349050	-35.316935	1.691622
-1270.399701	-30.485021	1.696627
-1274.460980	-31.233537	1.701632
-1278.264663	-39.117633	1.706637
-1282.174954	-17.809319	1.711642
-1285.462552	-38.977609	1.716646
-1289.286897	-38.139841	1.721651
-1292.975834	-33.203368	1.726656
-1296.735610	-45.971728	1.731661
-1301.180356	-28.403347	1.736666
-1304.742074	-32.148990	1.741670
-1308.516063	-38.640677	1.746675
-1312.101148	-34.614886	1.751680
-1315.434555	-38.639894	1.756685
-1319.391898	-26.911395	1.761690
-1323.150859	-32.404149	1.766694
-1327.031523	-27.107365	1.771699
-1330.860510	-27.011493	1.776704
-1334.484844	-41.524995	1.781709
-1338.541695	-31.212339	1.786714
-1342.378783	-32.882827	1.791718
-1346.181875	-26.343237	1.796723
-1349.804065	-28.841283	1.801728
-1353.277973	-34.715493	1.806733
-1357.229549	-25.031483	1.811738
-1360.690943	-50.765240	1.816742
-1364.562236	-27.507743	1.821747
-1368.667891	-32.870803	1.826752
-1372.076034	-44.041186	1.831757
-1375.829382	-21.592559	1.836762
-1379.339795	-34.211481	1.841766
-1383.182463	-35.223450	1.846771
-1387.271350	-31.039618	1.851776
-1391.009472	-35.819692	1.856781
-1394.956013	-28.292014	1.861786
-1398.425991	-46.695028	1.866790
-1402.275789	-32.356553	1.871795
-1405.658880	-39.997124	1.876800
-1409.671044	-34.343279	1.881805
-1413.894752	-27.360941	1.886810
-1417.499971	-28.270531	1.891814
-1421.193109	-29.385222	1.896819
-1424.906664	-32.183892	1.901824
-1428.247717	-40.646402	1.906829
-1432.411849	-33.113784	1.911834
-1436.026406	-33.621323	1.916838
-1439.833673	-27.309563	1.921843
-1443.687714	-30.082553	1.926848
-1447.297636	-34.682799	1.931853
-1451.510283	-40.077454	1.936858
-1454.784332	-40.917018	1.941862
-1458.732994	-34.364982	1.946867
-1462.520026	-29.727912	1.951872
-1466.331140	-32.126133	1.956877
-1470.307688	-21.603775	1.961882
-1473.422993	-36.435087	1.966886
-1477.502550	-30.924868	1.971891
-1481.335802	-37.916097	1.976896
-1484.936005	-30.076325	1.981901
-1488.751466	-22.407065	1.986906
-1492.187096	-31.786266	1.991910
-1496.182077	-44.253268	1.996915
-1500.207487	-32.991314	2.006912
-1501.549491	-29.708307	2.016909
-1498.828788	-31.152648	2.026906
-1495.814331	-34.055557	2.036902
-1493.747949	-35.499308	2.046899
-1492.007736	-42.139050	2.056896
-1490.031334	-29.888887	2.066893
-1488.044610	-29.583097	2.076890
-1486.053963	-33.957764	2.086886
-1484.107295	-27.552618	2.096883
-1482.447250	-27.971321	2.106880
-1480.237024	-31.910639	2.116877
-1478.370124	-34.544491	2.126874
-1476.996108	-30.485440	2.136870
-1474.979024	-28.461930	2.146867
-1472.871704	-33.063685	2.156864
-1470.976822	-26.877593	2.166861
-1468.881076	-33.286900	2.176858
-1467.013814	-37.423904	2.186854
-1465.440244	-31.663181	2.196851
-1463.486388	-27.144362	2.206848
-1461.291104	-27.375613	2.216845
-1459.726415	-29.927900	2.226842
-1458.065805	-20.982271	2.236838
-1456.037237	-29.810725	2.246835
-1453.837718	-26.532772	2.256832
-1452.029072	-35.112853	2.266829
-1450.043596	-29.555439	2.276826
-1448.335422	-31.696500	2.286822
-1446.404050	-27.952459	2.296819
-1444.512795	-33.888489	2.306816
-1442.735470	-28.844033	2.316813
-1440.550551	-38.340115	2.326810
-1439.011009	-29.138256	2.336806
-1437.172193	-34.472220	2.346803
-1435.198605	-43.364475	2.356800
-1433.296176	-27.066765	2.366797
-1431.271479	-31.844721	2.376794
-1429.503186	-37.142124	2.386790
-1427.412166	-37.756107	2.396787
-1425.732047	-35.820700	2.406784
-1423.791038	-32.766579	2.416781
-1422.192014	-45.280822	2.426778
-1420.311138	-32.497421	2.436774
-1417.767482	-38.984716	2.446771
-1416.305560	-33.337127	2.456768
-1414.621402	-25.134157	2.466765
-1412.677399	-32.430140	2.476762
-1410.857580	-44.867628	2.486758
-1408.818831	-35.115703	2.496755
-1406.858845	-36.090779	2.506752
-1405.084406	-39.227646	2.516749
-1403.345698	-34.398021	2.526746
-1401.186600	-36.551248	2.536742
-1399.197317	-33.088008	2.546739
-1397.738817	-34.083833	2.556736
-1395.527091	-35.561820	2.566733
-1393.693662	-32.970432	2.576730
-1392.056684	-33.080651	2.586726
-1390.181545	-32.797962	2.596723
-1388.163535	-42.185172	2.606720
-1386.334826	-27.410294	2.616717
-1384.316968	-35.256482	2.626714
-1382.589244	-31.585566	2.636710
-1380.505217	-48.372549	2.646707
-1378.655658	-43.123302	2.656704
-1377.020748	-30.068381	2.666701
-1374.987445	-39.191198	2.676698
-1373.371623	-26.333734	2.686694
-1371.104430	-36.992364	2.696691
-1369.182847	-29.964172	2.706688
-1367.468398	-38.701211	2.716685
-1365.842268	-31.579928	2.726682
-1364.085683	-35.969126	2.736678
-1361.859743	-42.257082	2.746675
-1359.899857	-37.087057	2.756672
-1357.787338	-34.425060	2.766669
-1356.183019	-34.209510	2.776666
-1354.278264	-28.095946	2.786662
-1352.646184	-35.809299	2.796659
-1350.715800	-29.513526	2.806656
-1348.376686	-31.722364	2.816653
-1346.864068	-35.943025	2.826650
-1344.961108	-25.675098	2.836646
-1342.983425	-37.329427	2.846643
-1341.233335	-31.385297	2.856640
-1339.539847	-38.195871	2.866637
-1337.799811	-27.895542	2.876634
-1335.288357	-36.556470	2.886630
-1333.553366	-31.906188	2.896627
-1331.768428	-29.889597	2.906624
-1329.784993	-36.555534	2.916621
-1328.055475	-29.578661	2.926618
-1326.263937	-39.875329	2.936614
-1323.918162	-39.307936	2.946611
-1322.474710	-35.629363	2.956608
-1320.690077	-35.341603	2.966605
-1318.859698	-36.180599	2.976602
-1316.652447	-33.611094	2.986598
-1315.051452	-34.852301	2.996595
-1313.145225	-38.526494	3.006592
-1311.461836	-37.974634	3.016589
-1309.007234	-32.710072	3.026586
-1307.312287	-36.197289	3.036582
-1305.580819	-36.567300	3.046579
-1303.689823	-36.416548	3.056576
-1301.834201	-26.439415	3.066573
-1299.929189	-25.531455	3.076570
-1297.874146	-43.772642	3.086566
-1296.101450	-29.730794	3.096563
-1294.308999	-37.062426	3.106560
-1292.690291	-37.927519	3.116557
-1290.791407	-29.956181	3.126554
-1288.447599	-35.127715	3.136550
-1286.822105	-38.856424	3.146547
-1284.939468	-40.213740	3.156544
-1282.653731	-32.703776	3.166541
-1281.105833	-41.691985	3.176538
-1279.361072	-40.954142	3.186534
-1277.622546	-36.819101	3.196531
-1275.397939	-37.520642	3.206528
-1273.382991	-38.224939	3.216525
-1271.828899	-34.511937	3.226522
-1269.888013	-26.389411	3.236518
-1268.098084	-34.197448	3.246515
-1266.159264	-39.900963	3.256512
-1264.071944	-35.592796	3.266509
-1262.394300	-43.589688	3.276506
-1260.365464	-43.100975	3.286502
-1258.463811	-37.356293	3.296499
-1257.009280	-35.915163	3.306496
-1254.936994	-31.729313	3.316493
-1252.992394	-39.791031	3.326490
-1250.850166	-37.983134	3.336486
-1249.246922	-40.129362	3.346483
-1247.377436	-38.961472	3.356480
-1245.239052	-37.269792	3.366477
-1243.646635	-41.166856	3.376474
-1241.928258	-32.533450	3.386470
-1239.757199	-36.369966	3.396467
-1237.924581	-33.923579	3.406464
-1236.094107	-37.928209	3.416461
-1234.264019	-26.694864	3.426458
-1232.452185	-29.164982	3.436454
-1230.433073	-33.905563	3.446451
-1228.303970	-33.540232	3.456448
-1226.717517	-36.597939	3.466445
-1224.913750	-35.204783	3.476442
-1222.824638	-36.214579	3.486438
-1220.847146	-33.679261	3.496435
-1219.169294	-36.238449	3.506432
-1217.720076	-37.011632	3.516429
-1215.725197	-30.249232	3.526426
-1213.472823	-32.369848	3.536422
-1211.442728	-35.015398	3.546419
-1209.853731	-30.640064	3.556416
-1207.927303	-25.938211	3.566413
-1205.944595	-35.818567	3.576410
-1204.027153	-29.590061	3.586406
-1202.315747	-30.269406	3.596403
-1200.449052	-32.331450	3.606400
-1198.819189	-32.410395	3.616397
-1196.754506	-33.504677	3.626394
-1194.567846	-34.206385	3.636390
-1192.920247	-36.680190	3.646387
-1191.143551	-31.291228	3.656384
-1189.330888	-27.976372	3.666381
-1187.324167	-34.811709	3.676378
-1185.576968	-32.119512	3.686374
-1183.590689	-28.600335	3.696371
-1181.576790	-27.897589	3.706368
-1179.742717	-33.664802	3.716365
-1177.867259	-28.998976	3.726362
-1175.880669	-33.074331	3.736358
-1174.184319	-27.411979	3.746355
-1172.163505	-25.991934	3.756352
-1170.347639	-34.422982	3.766349
-1168.952887	-22.477306	3.776346
-1166.732987	-27.722055	3.786342
-1164.573028	-28.594720	3.796339
-1162.998006	-24.070276	3.806336
-1161.153662	-26.709747	3.816333
-1159.015922	-31.545040	3.826330
-1157.034840	-29.256546	3.836326
-1155.179508	-26.478998	3.846323
-1153.571722	-31.204229	3.856320
-1151.831524	-33.028107	3.866317
-1149.853904	-24.104530	3.876314
-1148.106578	-32.993529	3.886310
-1145.939745	-31.607877	3.896307
-1143.931167	-31.670011	3.906304
-1142.274047	-32.932713	3.916301
-1140.375540	-29.431032	3.926298
-1138.488001	-34.860991	3.936294
-1136.652844	-36.437954	3.946291
-1134.696076	-34.552907	3.956288
-1132.781497	-30.853271	3.966285
-1130.891523	-34.922605	3.976282
-1129.316192	-31.440259	3.986278
-1127.212590	-41.008327	3.996275
-1125.184142	-36.594297	4.006272
-1123.758319	-36.830012	4.016269
-1121.834284	-47.204579	4.026266
-1119.620012	-38.997770	4.036262
-1117.728526	-37.743296	4.046259
-1115.866156	-36.211013	4.056256
-1114.370227	-34.024859	4.066253
-1112.422013	-43.029651	4.076250
-1110.530152	-33.645495	4.086246
-1108.395008	-29.578506	4.096243
-1106.360688	-33.598285	4.106240
-1104.842559	-29.525736	4.116237
-1102.960322	-29.764985	4.126234
-1101.108560	-26.454732	4.136230
-1098.872505	-34.848746	4.146227
-1096.824248	-31.712027	4.156224
-1095.503460	-34.452421	4.166221
-1093.362707	-36.056134	4.176218
-1091.574016	-34.499414	4.186214
-1089.857795	-31.603245	4.196211
-1087.820299	-31.444175	4.206208
-1085.810182	-27.546631	4.216205
-1084.044925	-35.429540	4.226202
-1082.334526	-33.309252	4.236198
-1080.333498	-27.700303	4.246195
-1078.407744	-31.134289	4.256192
-1076.515498	-33.745043	4.266189
-1074.783015	-40.544314	4.276186
-1072.599365	-33.447254	4.286182
-1070.816221	-36.447906	4.296179
-1069.114723	-32.761497	4.306176
-1067.342725	-35.869307	4.316173
-1065.445332	-37.490907	4.326170
-1063.477184	-34.087141	4.336166
-1061.667937	-30.102182	4.346163
-1059.873729	-31.339389	4.356160
-1057.281252	-34.774221	4.366157
-1055.987573	-29.955231	4.376154
-1054.329585	-29.549115	4.386150
-1052.094671	-27.632701	4.396147
-1050.142430	-30.298820	4.406144
-1048.398154	-37.339954	4.416141
-1046.580440	-33.659486	4.426138
-1044.618355	-37.694500	4.436134
-1042.741341	-40.845930	4.446131
-1040.981943	-40.154457	4.456128
-1039.192884	-34.359993	4.466125
-1037.294255	-33.548687	4.476122
-1035.222128	-33.339849	4.486118
-1033.363490	-36.488334	4.496115
-1031.452357	-36.193744	4.506112
-1029.607948	-29.896561	4.516109
-1027.960464	-31.342373	4.526106
-1025.723313	-38.203386	4.536102
-1023.979305	-38.226258	4.546099
-1022.354033	-36.401773	4.556096
-1020.227232	-33.271232	4.566093
-1018.483887	-38.273838	4.576090
-1016.716802	-32.856355	4.586086
-1014.934365	-33.581661	4.596083
-1012.601794	-44.378326	4.606080
-1010.590747	-40.059300	4.616077
-1009.145607	-35.869227	4.626074
-1007.216495	-43.956703	4.636070
-1005.281501	-42.612783	4.646067
-1003.290250	-44.721434	4.656064
-1001.557605	-39.257382	4.666061
-999.455084	-36.625028	4.676058
-997.639672	-40.581283	4.686054
-996.106169	-38.281065	4.696051
-993.794511	-42.485626	4.706048
-992.121669	-45.039118	4.716045
-990.424849	-37.524653	4.726042
-988.752951	-39.800106	4.736038
-986.332040	-33.632982	4.746035
-984.428829	-43.432563	4.756032
-982.546925	-41.649094	4.766029
-981.151267	-41.309916	4.776026
-978.942796	-31.519971	4.786022
-977.144794	-41.594818	4.796019
-975.585271	-41.733409	4.806016
-972.956577	-37.611018	4.816013
-971.250158	-30.825942	4.826010
-969.663053	-40.916002	4.836006
-967.845720	-42.249992	4.846003
-965.851962	-41.157008	4.856000
-964.163824	-37.035765	4.865997
-962.500804	-35.094120	4.875994
-960.556930	-41.279772	4.885990
-958.202512	-40.937594	4.895987
-955.985967	-40.327058	4.905984
-954.603151	-34.729655	4.915981
-952.724574	-27.228432	4.925978
-950.842705	-33.216275	4.935974
-949.049026	-37.355330	4.945971
-947.140841	-36.752314	4.955968
-945.115549	-39.002147	4.965965
-943.400569	-31.187396	4.975962
-941.567737	-34.680622	4.985958
-939.602724	-38.228140	4.995955
-937.827788	-45.463567	5.005952
-936.040484	-36.000956	5.015949
-933.864425	-40.594292	5.025946
-932.108583	-41.968947	5.035942
-930.004913	-40.538255	5.045939
-928.533716	-43.904170	5.055936
-926.426518	-40.404103	5.065933
-924.583799	-36.530172	5.075930
-922.441522	-37.248213	5.085926
-920.696264	-35.774411	5.095923
-918.989860	-37.655873	5.105920
-917.318168	-40.624380	5.115917
-915.016358	-30.157735	5.125914
-913.395200	-35.835448	5.135910
-911.723662	-31.133631	5.145907
-909.518894	-33.415291	5.155904
-907.701484	-35.993421	5.165901
-905.924137	-38.877766	5.175898
-903.997996	-37.630237	5.185894
-902.088069	-42.296250	5.195891
-899.948372	-47.073209	5.205888
-898.329821	-43.624454	5.215885
-896.506311	-38.106952	5.225882
-894.608138	-37.001781	5.235878
-892.765651	-40.618088	5.245875
-890.960000	-32.340965	5.255872
-888.727217	-36.224933	5.265869
-886.991381	-38.085815	5.275866
-885.620719	-34.902141	5.285862
-883.264212	-31.940826	5.295859
-881.408978	-46.073059	5.305856
-879.397990	-42.147052	5.315853
-877.509887	-38.828217	5.325850
-875.895353	-30.078431	5.335846
-873.769523	-37.597283	5.345843
-871.764397	-35.596588	5.355840
-870.379346	-34.425146	5.365837
-868.227275	-32.710039	5.375834
-866.539703	-46.509150	5.385830
-864.655139	-38.757767	5.395827
-862.484563	-30.736325	5.405824
-860.778212	-43.559519	5.415821
-859.251713	-39.113941	5.425818
-857.224218	-38.900968	5.435814
-855.119724	-38.045059	5.445811
-853.325519	-33.593329	5.455808
-851.144630	-34.795887	5.465805
-849.235915	-35.193898	5.475802
-847.586870	-37.874536	5.485798
-845.916037	-39.331850	5.495795
-844.024029	-32.620552	5.505792
-842.131748	-33.608018	5.515789
-839.941067	-43.245041	5.525786
-838.321532	-34.012883	5.535782
-836.474714	-33.177340	5.545779
-834.519573	-40.057836	5.555776
-832.705111	-35.314074	5.565773
-830.959218	-34.145033	5.575770
-828.750582	-40.151865	5.585766
-826.915834	-37.920216	5.595763
-825.106174	-34.287226	5.605760
-823.108441	-38.240923	5.615757
-821.437871	-32.702065	5.625754
-819.652547	-31.174593	5.635750
-817.596536	-38.994859	5.645747
-815.737114	-34.804570	5.655744
-813.568230	-32.717900	5.665741
-812.031555	-31.829601	5.675738
-810.243205	-33.463567	5.685734
-808.378701	-36.810182	5.695731
-806.480111	-44.106339	5.705728
-804.444352	-35.581725	5.715725
-802.756818	-38.265328	5.725722
-800.874696	-37.590133	5.735718
-798.859322	-31.034301	5.745715
-796.798309	-45.924092	5.755712
-795.021767	-34.228650	5.765709
-793.401120	-44.137660	5.775706
-791.359330	-34.655604	5.785702
-789.599014	-31.256269	5.795699
-787.469760	-36.882494	5.805696
-785.677775	-39.832247	5.815693
-784.068079	-32.968405	5.825690
-782.147133	-36.924006	5.835686
-780.125485	-38.200515	5.845683
-778.199514	-41.122734	5.855680
-776.255316	-38.619599	5.865677
-774.460198	-32.633258	5.875674
-772.584157	-31.884438	5.885670
-770.449257	-34.633212	5.895667
-769.047710	-33.552764	5.905664
-767.112388	-22.275813	5.915661
-764.786426	-39.356825	5.925658
-763.291402	-31.914128	5.935654
-761.317012	-44.251173	5.945651
-759.444668	-30.272128	5.955648
-757.338698	-34.080446	5.965645
-756.123513	-38.895826	5.975642
-754.072493	-32.705640	5.985638
-751.949445	-32.916784	5.995635
-749.782658	-38.223721	6.005632
-748.347839	-38.310651	6.015629
-746.487649	-31.298927	6.025626
-744.559354	-33.302570	6.035622
-742.436405	-31.900051	6.045619
-740.635629	-33.758577	6.055616
-738.875495	-29.015525	6.065613
-737.030046	-38.579921	6.075610
-735.302227	-23.920924	6.085606
-732.954204	-30.758354	6.095603
-731.224178	-27.917800	6.105600
-729.367993	-26.682627	6.115597
-727.553280	-28.592317	6.125594
-725.619756	-35.638221	6.135590
-723.898700	-30.059988	6.145587
-722.051402	-35.983718	6.155584
-719.995696	-27.500100	6.165581
-717.969955	-22.474224	6.175578
-716.380436	-20.418022	6.185574
-714.609356	-29.304225	6.195571
-712.534132	-42.874688	6.205568
-710.614537	-28.470527	6.215565
-708.667843	-35.516944	6.225562
-706.945685	-26.368971	6.235558
-705.083347	-38.809650	6.245555
-703.526914	-23.065369	6.255552
-701.447739	-33.789698	6.265549
-699.030141	-37.478824	6.275546
-697.584811	-35.503777	6.285542
-695.491754	-40.208374	6.295539
-694.015178	-34.148956	6.305536
-691.854154	-40.236480	6.315533
-690.041407	-32.242942	6.325530
-688.311231	-37.304795	6.335526
-686.173737	-41.839648	6.345523
-684.621786	-32.407100	6.355520
-682.664631	-41.247223	6.365517
-680.262815	-41.278646	6.375514
-678.832408	-35.938137	6.385510
-677.153715	-34.931921	6.395507
-675.189416	-44.638418	6.405504
-672.862181	-39.093860	6.415501
-671.297028	-51.862796	6.425498
-669.645882	-38.325155	6.435494
-667.505138	-39.971117	6.445491
-665.599557	-46.114110	6.455488
-663.856650	-35.712616	6.465485
-661.797303	-37.433986	6.475482
-660.193321	-39.103114	6.485478
-657.789186	-38.335960	6.495475
-656.204979	-40.548227	6.505472
-654.438026	-28.461135	6.515469
-652.320300	-42.556227	6.525466
-650.695941	-40.661861	6.535462
-649.236140	-38.982771	6.545459
-646.695940	-37.301057	6.555456
-645.151007	-37.301312	6.565453
-643.135258	-49.586460	6.575450
-641.222333	-36.943230	6.585446
-639.173622	-39.125500	6.595443
-637.310375	-47.780060	6.605440
-635.572327	-37.991960	6.615437
-633.880942	-41.893398	6.625434
-631.910337	-35.676040	6.635430
-629.951141	-42.716498	6.645427
-628.154759	-35.509746	6.655424
-626.046460	-45.676573	6.665421
-624.555046	-43.745158	6.675418
-622.450687	-40.509609	6.685414
-620.807309	-43.607600	6.695411
-618.725420	-44.167302	6.705408
-616.880410	-39.423508	6.715405
-615.121221	-46.561468	6.725402
-612.876599	-40.228406	6.735398
-611.355114	-44.465831	6.745395
-609.255895	-38.008483	6.755392
-607.443107	-35.635784	6.765389
-605.425447	-42.575042	6.775386
-603.868310	-37.055789	6.785382
-602.039598	-44.009065	6.795379
-599.802909	-41.219363	6.805376
-598.094334	-52.089648	6.815373
-596.312222	-38.492345	6.825370
-594.308371	-46.274100	6.835366
-592.228835	-34.047429	6.845363
-590.680511	-45.529990	6.855360
-588.943077	-42.415785	6.865357
-586.898437	-39.608019	6.875354
-585.139864	-39.069224	6.885350
-583.013857	-33.375582	6.895347
-581.138826	-30.493346	6.905344
-579.128779	-41.182849	6.915341
-577.543665	-40.845278	6.925338
-575.390098	-37.546496	6.935334
-573.890025	-35.597483	6.945331
-571.906490	-35.325138	6.955328
-570.175287	-34.624068	6.965325
-567.947966	-42.503084	6.975322
-566.162180	-39.953939	6.985318
-564.455654	-42.144636	6.995315
-562.431061	-37.751582	7.005312
-560.529765	-38.703952	7.015309
-558.978071	-37.574734	7.025306
-556.990673	-41.581829	7.035302
-554.848649	-30.062975	7.045299
-552.790191	-40.019686	7.055296
-551.229534	-41.310779	7.065293
-549.312835	-40.861953	7.075290
-547.185766	-38.323102	7.085286
-545.500934	-43.994966	7.095283
-544.181624	-30.881032	7.105280
-541.659632	-40.076540	7.115277
-539.701916	-40.333713	7.125274
-538.371764	-49.679868	7.135270
-536.274938	-36.552771	7.145267
-534.058269	-37.197086	7.155264
-532.256678	-39.508733	7.165261
-530.871128	-40.833419	7.175258
-528.664104	-26.721303	7.185254
-526.843528	-38.091013	7.195251
-524.750794	-39.296560	7.205248
-522.963978	-42.291086	7.215245
-520.942527	-44.388377	7.225242
-519.729167	-36.911568	7.235238
-517.700776	-37.198960	7.245235
-515.539791	-32.592392	7.255232
-513.665303	-34.737254	7.265229
-511.743480	-41.200091	7.275226
-509.932725	-37.327030	7.285222
-507.999794	-43.390595	7.295219
-506.005876	-41.381477	7.305216
-504.248144	-32.984267	7.315213
-502.214194	-30.301029	7.325210
-500.838279	-34.908287	7.335206
-498.827619	-37.275410	7.345203
-496.637639	-34.471830	7.355200
-494.833715	-35.849111	7.365197
-493.014079	-30.370124	7.375194
-491.215477	-29.731866	7.385190
-489.616437	-29.246463	7.395187
-487.344810	-22.516537	7.405184
-485.186977	-33.182215	7.415181
-483.783837	-38.338535	7.425178
-481.802875	-27.153870	7.435174
-479.934415	-27.995145	7.445171
-477.899605	-27.255659	7.455168
-476.189693	-27.897928	7.465165
-474.341494	-34.669500	7.475162
-472.064124	-26.431041	7.485158
-470.414385	-32.569350	7.495155
-469.035581	-41.039060	7.505152
-466.660055	-36.809334	7.515149
-464.922081	-39.314452	7.525146
-463.238743	-36.188351	7.535142
-461.028096	-24.571412	7.545139
-459.039426	-40.459920	7.555136
-457.214840	-39.262116	7.565133
-455.744129	-33.613692	7.575130
-453.461212	-34.503771	7.585126
-451.874832	-31.278494	7.595123
-449.966090	-38.580756	7.605120
-448.155858	-35.043868	7.615117
-446.041658	-33.747048	7.625114
-444.018758	-31.303567	7.635110
-442.185635	-35.364880	7.645107
-440.260614	-38.930879	7.655104
-438.927543	-32.763106	7.665101
-436.891553	-38.956761	7.675098
-434.843748	-22.561272	7.685094
-432.956025	-28.270208	7.695091
-431.269717	-32.687006	7.705088
-428.974547	-29.424908	7.715085
-427.204742	-32.817694	7.725082
-425.778836	-26.165800	7.735078
-423.820439	-38.260069	7.745075
-421.561363	-27.907635	7.755072
-419.463308	-37.027434	7.765069
-418.089805	-35.414941	7.775066
-416.053322	-28.374242	7.785062
-414.064764	-28.337825	7.795059
-412.213181	-35.210944	7.805056
-410.569177	-38.855200	7.815053
-408.737613	-34.931696	7.825050
-406.738535	-34.729588	7.835046
-404.475768	-29.512339	7.845043
-403.061272	-29.706339	7.855040
-401.095826	-38.476534	7.865037
-399.276087	-28.690222	7.875034
-397.506189	-26.703656	7.885030
-395.372376	-28.119331	7.895027
-393.559391	-32.493176	7.905024
-391.585917	-32.367491	7.915021
-389.919879	-23.641335	7.925018
-388.000415	-26.186434	7.935014
-386.058262	-33.642405	7.945011
-384.323836	-37.705283	7.955008
-382.431667	-37.999230	7.965005
-380.548578	-34.300241	7.975002
-378.619099	-33.419117	7.984998
-376.705639	-30.290224	7.994995
-374.503487	-32.967289	8.004992
-372.933792	-39.770106	8.014989
-370.991573	-29.818595	8.024986
-369.358950	-27.685355	8.034982
-367.134234	-32.481756	8.044979
-365.197157	-30.547122	8.054976
-363.752569	-37.672582	8.064973
-362.093296	-40.220324	8.074970
-359.669856	-29.571972	8.084966
-357.995965	-38.248216	8.094963
-356.148350	-26.857408	8.104960
-354.129648	-39.212304	8.114957
-352.353276	-36.285709	8.124954
-350.377951	-29.426233	8.134950
-348.461488	-27.759866	8.144947
-346.747765	-27.895822	8.154944
-344.671265	-28.271273	8.164941
-342.728804	-31.530517	8.174938
-341.228906	-32.555993	8.184934
-339.293104	-34.232102	8.194931
-337.195493	-28.394746	8.204928
-335.549163	-30.436732	8.214925
-333.493818	-31.599830	8.224922
-331.603122	-29.760393	8.234918
-330.096977	-27.790085	8.244915
-327.666755	-25.280483	8.254912
-325.799489	-33.190234	8.264909
-324.071257	-26.644960	8.274906
-322.563246	-24.918098	8.284902
-320.432273	-22.607022	8.294899
-318.457429	-31.449712	8.304896
-316.556057	-31.959808	8.314893
-315.057921	-24.949906	8.324890
-312.848592	-35.683667	8.334886
-310.980390	-28.743897	8.344883
-309.066108	-29.020790	8.354880
-307.057310	-26.488098	8.364877
-305.532892	-34.598883	8.374874
-303.512467	-28.744436	8.384870
-301.816537	-25.553910	8.394867
-299.706083	-27.210504	8.404864
-298.023688	-29.198224	8.414861
-295.864023	-24.357554	8.424858
-294.258015	-28.303559	8.434854
-292.355193	-34.152167	8.444851
-290.399481	-37.896632	8.454848
-288.527619	-32.329502	8.464845
-286.457146	-31.971326	8.474842
-284.872938	-21.114702	8.484838
-282.817200	-31.468668	8.494835
-280.819477	-33.621975	8.504832
-279.140471	-32.557105	8.514829
-277.474335	-32.818043	8.524826
-275.646528	-30.153803	8.534822
-273.296048	-30.424511	8.544819
-271.697437	-27.649471	8.554816
-269.539658	-30.327255	8.564813
-267.899435	-21.814770	8.574810
-266.045285	-25.729319	8.584807
-263.981317	-24.787466	8.594803
-262.400435	-24.425325	8.604800
-260.288451	-27.428942	8.614797
-258.295501	-24.279480	8.624794
-256.675021	-21.223715	8.634791
-254.926167	-18.752111	8.644787
-252.736458	-23.980187	8.654784
-251.267517	-28.065336	8.664781
-248.969936	-18.696206	8.674778
-247.168088	-28.862783	8.684775
-245.543003	-25.210917	8.694771
-243.531860	-23.509051	8.704768
-241.592014	-26.646225	8.714765
-239.462641	-29.709440	8.724762
-237.993274	-23.166986	8.734759
-236.235725	-27.351876	8.744755
-233.894220	-21.532824	8.754752
-232.087915	-28.318070	8.764749
-230.029905	-22.439553	8.774746
-228.582540	-31.494822	8.784743
-226.776664	-27.698119	8.794739
-224.597687	-31.906056	8.804736
-222.985773	-29.963614	8.814733
-221.212811	-26.505856	8.824730
-219.042545	-25.964607	8.834727
-217.085280	-29.162961	8.844723
-215.339904	-24.295562	8.854720
-213.335474	-31.353990	8.864717
-211.588470	-23.966903	8.874714
-209.725604	-28.822255	8.884711
-207.707140	-26.324176	8.894707
-206.089216	-29.487308	8.904704
-204.119295	-22.101057	8.914701
-202.210386	-35.174101	8.924698
-200.249209	-35.321026	8.934695
-198.140769	-32.652568	8.944691
-196.503897	-31.195660	8.954688
-194.306690	-38.929034	8.964685
-193.035093	-32.759191	8.974682
-190.979857	-38.927305	8.984679
-189.243017	-39.011577	8.994675
-187.121330	-37.726773	9.004672
-185.007190	-43.370609	9.014669
-183.620602	-39.393277	9.024666
-181.760112	-41.270396	9.034663
-179.800789	-39.370739	9.044659
-177.754878	-42.145849	9.054656
-175.749476	-43.662414	9.064653
-174.056273	-47.314368	9.074650
-172.130429	-50.997131	9.084647
-170.388301	-40.293527	9.094643
-168.362354	-44.524358	9.104640
-166.831217	-41.935844	9.114637
-164.928143	-42.885030	9.124634
-162.712919	-42.726686	9.134631
-160.533537	-39.782155	9.144627
-158.833086	-38.150635	9.154624
-157.348123	-41.573562	9.164621
-155.231737	-41.293651	9.174618
-153.378871	-39.601189	9.184615
-151.492967	-40.029741	9.194611
-149.780503	-40.455876	9.204608
-147.863424	-48.738175	9.214605
-145.875251	-46.789411	9.224602
-144.151863	-47.687802	9.234599
-142.131700	-42.537368	9.244595
-140.269377	-43.838445	9.254592
-138.687512	-37.771767	9.264589
-136.628137	-39.088497	9.274586
-134.530110	-33.821007	9.284583
-132.799034	-35.085346	9.294579
-130.755441	-36.915858	9.304576
-129.034098	-41.783301	9.314573
-126.992905	-38.660374	9.324570
-125.435362	-38.491784	9.334567
-123.565531	-37.294626	9.344563
-121.536011	-48.293212	9.354560
-119.548956	-35.443429	9.364557
-117.755904	-46.775326	9.374554
-115.834807	-39.550157	9.384551
-113.849972	-40.403405	9.394547
-112.439155	-35.132027	9.404544
-110.570982	-38.511866	9.414541
-107.973644	-47.092153	9.424538
-106.572179	-38.612507	9.434535
-104.630009	-43.409382	9.444531
-102.732097	-48.677602	9.454528
-100.928205	-44.139978	9.464525
-99.130651	-43.477573	9.474522
-96.967540	-32.698971	9.484519
-95.354763	-38.269055	9.494515
-93.441919	-36.469276	9.504512
-91.339076	-38.672359	9.514509
-89.870567	-41.805259	9.524506
-87.862510	-36.697053	9.534503
-85.896562	-30.407412	9.544499
-83.971046	-36.537378	9.554496
-82.034790	-35.551308	9.564493
-80.475574	-35.877155	9.574490
-78.622306	-35.642036	9.584487
-76.279214	-35.300335	9.594483
-74.333198	-37.869953	9.604480
-72.618927	-38.271060	9.614477
-70.987358	-34.992730	9.624474
-69.136418	-42.086554	9.634471
-67.171077	-34.449987	9.644467
-65.064689	-37.697277	9.654464
-63.210256	-38.895987	9.664461
-61.473276	-34.156604	9.674458
-59.816388	-35.846415	9.684455
-57.946025	-36.488726	9.694451
-55.970328	-33.225816	9.704448
-54.004854	-39.008457	9.714445
-52.122519	-42.916291	9.724442
-50.333268	-28.656485	9.734439
-48.398751	-31.655293	9.744435
-46.325248	-35.014161	9.754432
-44.507722	-40.119521	9.764429
-42.711057	-34.475454	9.774426
-40.941105	-36.259078	9.784423
-38.872699	-41.549718	9.794419
-36.975523	-34.424870	9.804416
-35.195380	-34.321733	9.814413
-33.143274	-41.821828	9.824410
-31.767478	-33.795920	9.834407
-29.959900	-34.587665	9.844403
-27.464769	-30.946552	9.854400
-25.878562	-40.448592	9.864397
-23.808990	-38.541131	9.874394
-22.083661	-31.336750	9.884391
-20.310020	-35.827210	9.894387
-18.423359	-39.410454	9.904384
-16.390092	-40.099247	9.914381
-14.522560	-42.888398	9.924378
-12.674567	-38.165110	9.934375
-11.018683	-31.251214	9.944371
-9.235221	-25.807112	9.954368
-7.397304	-16.768602	9.964365
-6.243843	10.096164	9.974362
-4.556721	38.656877	9.984359
-2.911770	86.883614	9.994355
-1.398208	133.798851	10.004352
0.000000	188.075398	10.009357
0.225467	231.004445	10.014362
0.804811	253.519007	10.019367
1.298047	291.070770	10.024371
1.615454	308.905867	10.029376
2.179594	336.046557	10.034381
2.208853	348.384733	10.039386
2.451726	351.440093	10.044391
2.712762	373.641346	10.049395
2.761390	392.246391	10.054400
3.038385	392.722745	10.059405
2.797328	402.014855	10.064410
3.047896	410.605655	10.069415
3.499542	398.206779	10.074419
3.396382	408.555526	10.079424
3.120362	411.876597	10.084429
3.383296	416.466293	10.089434
3.578798	438.493597	10.094439
3.802235	435.387784	10.099443
3.488419	433.343805	10.104448
3.775043	440.110649	10.109453
3.809865	455.073649	10.114458
3.700649	453.720849	10.119463
4.025445	457.914338	10.124467
3.681643	453.408788	10.129472
3.543129	449.781969	10.134477
3.590526	460.428434	10.139482
4.020887	460.635899	10.144487
4.499739	468.423919	10.149491
4.042068	476.799728	10.154496
4.502915	468.887333	10.159501
4.265961	489.151280	10.164506
4.217828	475.070605	10.169511
4.503361	473.669027	10.174515
3.909790	468.135718	10.179520
4.373212	460.005297	10.184525
4.284883	474.898076	10.189530
4.561493	479.648037	10.194535
4.725752	477.789564	10.199539
4.333082	490.833833	10.204544
4.357275	482.604730	10.209549
4.571978	495.189417	10.214554
4.465021	495.326475	10.219559
4.466646	485.676981	10.224563
4.598091	504.063955	10.229568
4.432852	499.175092	10.234573
4.571870	492.578739	10.239578
4.682872	491.588200	10.244583
5.021633	501.644169	10.249587
4.699298	507.590396	10.254592
4.794929	495.505272	10.259597
4.780466	506.547993	10.264602
4.803512	517.248847	10.269607
5.235263	514.127134	10.274611
5.223085	531.532532	10.279616
5.281401	528.091916	10.284621
5.220889	536.451714	10.289626
5.185635	533.559036	10.294631
5.088054	526.856906	10.299635
5.134766	544.681858	10.304640
5.316963	537.750590	10.309645
5.418549	531.379388	10.314650
5.454777	542.984910	10.319655
5.507301	539.724989	10.324659
5.673473	539.881557	10.329664
5.685242	544.336317	10.334669
5.507851	546.804320	10.339674
5.380385	547.312082	10.344679
5.909258	533.353774	10.349683
5.793356	551.953731	10.354688
5.848484	534.923378	10.359693
5.616796	548.432453	10.364698
5.517764	556.208624	10.369703
5.734726	564.145706	10.374707
5.806010	564.389951	10.379712
6.011731	572.167980	10.384717
6.199478	583.847136	10.389722
6.206323	585.937248	10.394727
6.158389	577.694366	10.399731
5.917673	591.373655	10.404736
6.237355	592.272142	10.409741
6.180016	589.682599	10.414746
6.229804	595.479615	10.419751
6.201650	590.423772	10.424755
6.332780	600.694281	10.429760
6.244524	598.283134	10.434765
6.360115	596.482872	10.439770
6.223921	604.074184	10.444775
6.360410	608.679381	10.449779
6.502038	621.465070	10.454784
7.025629	622.884548	10.459789
6.797041	630.465381	10.464794
6.660091	641.657054	10.469799
6.842429	633.287521	10.474803
6.709832	626.830630	10.479808
6.831268	633.368447	10.484813
6.888773	638.525576	10.489818
6.778402	637.691767	10.494823
7.111625	640.180837	10.499827
6.608644	643.511356	10.504832
7.223624	634.181820	10.509837
7.091795	637.613983	10.514842
6.977604	647.478953	10.519847
7.448563	648.823250	10.524851
7.574564	663.182133	10.529856
7.300802	666.750486	10.534861
7.243770	668.607945	10.539866
7.330144	675.463614	10.544871
7.888252	673.712605	10.549875
7.660232	681.659231	10.554880
7.833734	678.081932	10.559885
7.540674	665.451534	10.564890
7.426490	669.164746	10.569895
7.834235	684.008570	10.574899
7.693664	685.948744	10.579904
7.798664	685.460627	10.584909
7.624060	687.385729	10.589914
7.911337	689.494202	10.594919
7.930772	688.474100	10.599923
7.783443	695.740802	10.604928
7.905448	692.821429	10.609933
7.865623	693.168557	10.614938
8.119055	692.521143	10.619943
7.808722	701.147971	10.624947
8.085832	701.468197	10.629952
7.818778	693.643408	10.634957
8.124710	709.241523	10.639962
8.143599	716.418642	10.644967
8.424148	725.036385	10.649971
8.159098	726.455517	10.654976
8.559176	722.217581	10.659981
8.629421	722.810508	10.664986
8.463309	727.833026	10.669991
8.583504	732.568597	10.674995
8.569132	733.649693	10.680000
8.382307	728.300562	10.685005
8.416947	739.857608	10.690010
8.547382	732.762613	10.695015
8.904781	725.647188	10.700019
8.296063	731.979816	10.705024
8.627451	755.676449	10.710029
8.810034	757.992447	10.715034
8.976416	754.152909	10.720039
9.174972	770.339087	10.725043
8.791382	763.464846	10.730048
9.208207	774.382202	10.735053
9.017738	764.728471	10.740058
8.863951	768.268249	10.745063
9.072175	764.891975	10.750067
9.050251	777.415303	10.755072
9.364586	769.232799	10.760077
9.236274	772.244955	10.765082
9.294105	780.595478	10.770087
9.537275	779.534950	10.775091
9.675884	796.900843	10.780096
9.722108	790.907374	10.785101
9.470847	775.113085	10.790106
9.436585	789.136528	10.795111
9.855054	791.425942	10.800115
10.001251	802.206712	10.805120
9.903631	795.558082	10.810125
9.716636	801.515956	10.815130
9.747474	795.499708	10.820135
10.070536	813.397605	10.825139
9.877831	809.585370	10.830144
10.160417	806.526816	10.835149
9.734343	805.069982	10.840154
9.899631	818.855036	10.845159
9.872084	810.422685	10.850163
9.839066	809.051389	10.855168
9.872709	818.435565	10.860173
9.884754	808.963971	10.865178
9.880190	819.745148	10.870183
10.903743	838.598960	10.875187
10.476082	829.717899	10.880192
10.389108	826.587401	10.885197
10.459015	828.921384	10.890202
10.442504	843.068206	10.895207
10.688606	843.710358	10.900211
10.659569	852.271903	10.905216
10.627001	853.903127	10.910221
11.128882	851.399379	10.915226
10.860160	844.863177	10.920231
10.777173	823.410553	10.925235
10.708989	839.707167	10.930240
10.915055	838.376580	10.935245
11.089273	848.459038	10.940250
10.957360	848.328838	10.945255
11.073766	852.667650	10.950259
11.082346	865.640363	10.955264
11.193678	850.650769	10.960269
11.027114	857.579988	10.965274
10.637988	849.262064	10.970279
11.033833	860.044055	10.975283
11.023894	859.320372	10.980288
11.094752	847.932784	10.985293
11.133495	850.818959	10.990298
11.140231	865.356342	10.995303
11.347558	862.117389	11.000307
11.329961	861.942144	11.005312
11.439740	872.640463	11.010317
11.502383	892.122301	11.015322
11.649555	891.603796	11.020327
11.812947	887.387798	11.025331
11.492923	889.807645	11.030336
11.550112	885.622782	11.035341
11.781589	892.461716	11.040346
11.428872	890.378142	11.045351
11.805022	878.197489	11.050355
11.744333	894.190186	11.055360
11.812431	894.354519	11.060365
11.651653	897.428651	11.065370
11.899990	888.548535	11.070375
12.238439	894.192390	11.075379
12.112306	922.145265	11.080384
12.152837	917.409522	11.085389
12.235074	910.888272	11.090394
12.133433	927.523069	11.095399
12.665285	921.373232	11.100403
12.524027	915.748673	11.105408
12.635026	916.002360	11.110413
12.618481	926.514283	11.115418
12.549708	910.542498	11.120423
13.004398	897.265114	11.125427
12.279414	900.426092	11.130432
12.626612	895.270844	11.135437
12.458812	904.072180	11.140442
12.550405	914.078763	11.145447
12.999456	913.031119	11.150451
12.994307	916.100931	11.155456
12.917192	923.821761	11.160461
12.949510	920.476666	11.165466
12.869438	930.219687	11.170471
13.122822	918.607380	11.175475
13.008256	930.262497	11.180480
13.141795	928.296901	11.185485
12.989679	930.525963	11.190490
12.609211	938.553818	11.195495
12.939948	930.095786	11.200499
12.881943	933.423199	11.205504
12.921259	934.213463	11.210509
12.956212	935.472792	11.215514
13.588533	936.758261	11.220519
13.818744	940.609001	11.225523
13.163888	945.581817	11.230528
13.338383	944.196331	11.235533
13.660192	948.038769	11.240538
13.581562	955.597426	11.245543
13.737482	950.425360	11.250547
13.580392	972.471871	11.255552
13.990433	961.760244	11.260557
13.775344	959.922797	11.265562
13.668988	975.102825	11.270567
13.902371	965.550088	11.275571
13.718885	962.498036	11.280576
13.909008	959.540935	11.285581
14.029566	968.647985	11.290586
13.994957	977.054369	11.295591
14.002160	978.603567	11.300595
13.903224	976.400648	11.305600
13.825888	968.488674	11.310605
14.190643	964.986457	11.315610
13.963830	969.859463	11.320615
14.217500	967.641302	11.325619
14.317388	981.047423	11.330624
14.116512	966.273097	11.335629
14.588188	972.709466	11.340634
14.431558	989.144940	11.345639
14.909446	984.941828	11.350643
14.426987	986.608559	11.355648
14.493299	988.252412	11.360653
15.022334	991.296957	11.365658
14.816799	994.632148	11.370663
14.958620	978.891633	11.375667
14.587550	980.042261	11.380672
14.520781	979.452220	11.385677
14.903257	990.860938	11.390682
14.813459	1001.829317	11.395687
15.153350	1002.844461	11.400691
15.177366	996.113255	11.405696
14.965796	1003.678950	11.410701
15.027627	999.832371	11.415706
14.905835	999.098136	11.420711
15.403688	1003.948603	11.425715
15.083726	1003.804240	11.430720
14.934225	991.015035	11.435725
15.376416	1004.057481	11.440730
14.737789	1011.448442	11.445735
15.177823	1004.423782	11.450739
15.064272	1012.082660	11.455744
15.149479	1008.432630	11.460749
15.398139	1016.265553	11.465754
15.471825	1022.703925	11.470759
15.800928	1030.241739	11.475763
15.535724	1041.697038	11.480768
15.665697	1036.540120	11.485773
15.814700	1035.710646	11.490778
15.612323	1034.259107	11.495783
15.711306	1030.616336	11.500787
15.738138	1033.129117	11.505792
15.789400	1034.242345	11.510797
15.865428	1033.448168	11.515802
15.725387	1045.624701	11.520807
16.002979	1026.817262	11.525811
15.912335	1034.153941	11.530816
15.961078	1040.312437	11.535821
15.917503	1056.162228	11.540826
16.288610	1074.976917	11.545831
16.441634	1068.056359	11.550835
16.142631	1069.312197	11.555840
16.455302	1074.729990	11.560845
16.419218	1070.632495	11.565850
16.602758	1059.233076	11.570855
16.740418	1057.169030	11.575859
16.612245	1066.101343	11.580864
16.995781	1066.086046	11.585869
16.731490	1060.187731	11.590874
16.551628	1061.465567	11.595879
16.900371	1055.215568	11.600883
16.826717	1066.285503	11.605888
16.591099	1067.297832	11.610893
16.409010	1070.722344	11.615898
16.155684	1069.089685	11.620903
16.646822	1059.560430	11.625907
17.009078	1069.680860	11.630912
16.936164	1061.206712	11.635917
16.809301	1075.522757	11.640922
16.779943	1072.286816	11.645927
17.520761	1083.611639	11.650931
16.950555	1084.343012	11.655936
17.455463	1085.885374	11.660941
17.391061	1084.164228	11.665946
17.372762	1103.474750	11.670951
17.480568	1086.465311	11.675955
17.044455	1081.759812	11.680960
17.281823	1088.285650	11.685965
17.505596	1088.390459	11.690970
17.267495	1100.532215	11.695975
17.597169	1102.299658	11.700979
17.407865	1097.002828	11.705984
17.435538	1097.012755	11.710989
17.580118	1096.746980	11.715994
17.242950	1103.014372	11.720999
17.583385	1104.442617	11.726003
17.964362	1118.133624	11.731008
17.942987	1123.681994	11.736013
18.275215	1112.984246	11.741018
17.873406	1112.796165	11.746023
17.929689	1103.845624	11.751027
17.894399	1118.195991	11.756032
18.214465	1121.013689	11.761037
18.235637	1132.101666	11.766042
17.785727	1134.786710	11.771047
18.303779	1125.016566	11.776051
18.237600	1127.216179	11.781056
18.476301	1136.637241	11.786061
18.464888	1132.004336	11.791066
18.278471	1137.069659	11.796071
18.424217	1133.810505	11.801075
18.446972	1138.815653	11.806080
18.635701	1130.611980	11.811085
18.337343	1130.883658	11.816090
18.373183	1139.398752	11.821095
18.498205	1131.922786	11.826099
18.765064	1124.473088	11.831104
19.058575	1135.594900	11.836109
18.632780	1145.953056	11.841114
18.661047	1143.835481	11.846119
18.672210	1129.560200	11.851123
18.746861	1149.277021	11.856128
19.130349	1154.257752	11.861133
19.339176	1152.448858	11.866138
19.073723	1155.673789	11.871143
19.360090	1154.286209	11.876147
19.288821	1147.000826	11.881152
19.148936	1140.513327	11.886157
18.983807	1136.657181	11.891162
18.854808	1155.435048	11.896167
19.114939	1147.126931	11.901171
19.310976	1154.870548	11.906176
19.067713	1141.668791	11.911181
19.327952	1163.902925	11.916186
19.334562	1154.069256	11.921191
19.351389	1149.633699	11.926195
19.695624	1153.911029	11.931200
19.577502	1145.152293	11.936205
19.530800	1155.913632	11.941210
19.658623	1178.583667	11.946215
19.909897	1166.503123	11.951219
19.645253	1184.466839	11.956224
19.849095	1190.212711	11.961229
20.142422	1185.651033	11.966234
19.924990	1189.805067	11.971239
19.960489	1189.012615	11.976243
19.829517	1191.126374	11.981248
20.155068	1194.236539	11.986253
20.041305	1180.102567	11.991258
20.290044	1176.776510	11.996263
20.541099	1192.049571	12.001267
20.458504	1178.588752	12.006272
20.590618	1178.793342	12.011277
20.738968	1176.505213	12.016282
20.415055	1171.273984	12.021287
20.075448	1162.802891	12.026291
19.978129	1164.282044	12.031296
20.031839	1175.199276	12.036301
20.362295	1170.879274	12.041306
20.003140	1194.481762	12.046311
20.634705	1174.857541	12.051315
20.503460	1182.296969	12.056320
20.330497	1175.570291	12.061325
20.623648	1181.101631	12.066330
20.332098	1163.681118	12.071335
20.459460	1157.575203	12.076339
20.176449	1153.010846	12.081344
20.319442	1151.469509	12.086349
20.487656	1146.104593	12.091354
20.335976	1148.888731	12.096359
20.527314	1142.876701	12.101363
20.170915	1159.847305	12.106368
20.224530	1154.940656	12.111373
20.709872	1148.074289	12.116378
19.877879	1161.009450	12.121383
20.113181	1157.163546	12.126387
20.149045	1147.219554	12.131392
20.075817	1157.641333	12.136397
20.528431	1167.200191	12.141402
20.469059	1179.963239	12.146407
20.480092	1157.287119	12.151411
20.491319	1158.881428	12.156416
20.168750	1163.895934	12.161421
20.394689	1154.585547	12.166426
20.192020	1153.566147	12.171431
20.475115	1149.769394	12.176435
20.275430	1155.281560	12.181440
20.351338	1155.901988	12.186445
20.674463	1161.461656	12.191450
20.251825	1162.115874	12.196455
20.301694	1153.060665	12.201459
20.364690	1158.505700	12.206464
20.163013	1155.981658	12.211469
20.421826	1161.956881	12.216474
20.020697	1153.358405	12.221479
20.457371	1161.276540	12.226483
20.149000	1164.429467	12.231488
20.295828	1160.763262	12.236493
20.565535	1151.460088	12.241498
20.515958	1159.208191	12.246503
20.502269	1158.023022	12.251507
20.339087	1163.496251	12.256512
20.547436	1164.871451	12.261517
20.576532	1160.269924	12.266522
20.457157	1162.006497	12.271527
20.667612	1163.874970	12.276531
20.588930	1161.681408	12.281536
20.444855	1160.312023	12.286541
20.474020	1142.096022	12.291546
20.153642	1152.388479	12.296551
20.327863	1140.378597	12.301555
20.129080	1145.751837	12.306560
20.347418	1160.239994	12.311565
20.417418	1146.475730	12.316570
20.478358	1137.841407	12.321575
20.542878	1133.607992	12.326579
20.404722	1136.779496	12.331584
20.571937	1145.210557	12.336589
20.764281	1135.217958	12.341594
20.425805	1148.367713	12.346599
20.615660	1139.689171	12.351603
20.597899	1147.130980	12.356608
20.380164	1139.460515	12.361613
20.419855	1147.055594	12.366618
20.202331	1151.348409	12.371623
20.609392	1148.866046	12.376627
20.670072	1145.538453	12.381632
20.052171	1128.857622	12.386637
20.451928	1123.932042	12.391642
20.185300	1132.618387	12.396647
20.265806	1139.781155	12.401651
20.382338	1141.486404	12.406656
20.198064	1129.789192	12.411661
20.466994	1140.086992	12.416666
20.147314	1134.583852	12.421671
20.573789	1130.934551	12.426675
20.405079	1118.992004	12.431680
20.170201	1123.787496	12.436685
20.367318	1113.931352	12.441690
20.311704	1117.315199	12.446695
20.280976	1121.068831	12.451699
19.959228	1119.928073	12.456704
20.212436	1138.078800	12.461709
20.341469	1136.809363	12.466714
19.994956	1146.170809	12.471719
20.657704	1145.620520	12.476723
20.183602	1156.700782	12.481728
20.187922	1158.934888	12.486733
20.481534	1158.853507	12.491738
20.369121	1152.498822	12.496743
20.131286	1153.177181	12.501747
20.341623	1151.538365	12.506752
20.441299	1152.992403	12.511757
20.397701	1149.224105	12.516762
20.256033	1161.402572	12.521767
20.392494	1153.792300	12.526771
20.382906	1156.219445	12.531776
20.254752	1141.781862	12.536781
20.620542	1149.018983	12.541786
20.372799	1134.004368	12.546791
20.108385	1129.509595	12.551795
20.593571	1130.247672	12.556800
20.476466	1135.913824	12.561805
20.299004	1129.862851	12.566810
20.401608	1121.966248	12.571815
20.411494	1118.222544	12.576819
20.395460	1126.731712	12.581824
20.359023	1137.906157	12.586829
20.644352	1127.040830	12.591834
20.225835	1136.189818	12.596839
20.465604	1126.804699	12.601843
20.612902	1132.250470	12.606848
20.457992	1127.646764	12.611853
20.301937	1132.147398	12.616858
20.398333	1133.657153	12.621863
20.511168	1121.313287	12.626867
20.219963	1136.532431	12.631872
20.358702	1131.612211	12.636877
20.719169	1133.404711	12.641882
20.798394	1135.139565	12.646887
20.538840	1122.052393	12.651891
20.227792	1105.928218	12.656896
20.165289	1102.555627	12.661901
20.390323	1094.615853	12.666906
19.992976	1096.254826	12.671911
20.085660	1093.562410	12.676915
20.312331	1106.478472	12.681920
20.134285	1124.647508	12.686925
20.370002	1117.716890	12.691930
20.298394	1128.139967	12.696935
20.378307	1120.234367	12.701939
20.478013	1124.098088	12.706944
20.303957	1111.658060	12.711949
20.262964	1110.084572	12.716954
19.972929	1111.250669	12.721959
20.448955	1119.723924	12.726963
20.490581	1131.756429	12.731968
20.218779	1134.771046	12.736973
20.262403	1125.352558	12.741978
20.467543	1132.817155	12.746983
20.564613	1118.567607	12.751987
20.144465	1111.765265	12.756992
20.289786	1104.240342	12.761997
20.398805	1096.449966	12.767002
20.087042	1107.201507	12.772007
20.109707	1117.256286	12.777011
20.311750	1124.500589	12.782016
20.173748	1140.950611	12.787021
20.624043	1124.545693	12.792026
20.443841	1127.558314	12.797031
20.416186	1119.286657	12.802035
20.180672	1109.078460	12.807040
20.084771	1107.182555	12.812045
20.553308	1118.407329	12.817050
20.368139	1115.435941	12.822055
20.308920	1099.717901	12.827059
20.445619	1105.256820	12.832064
20.104774	1106.030458	12.837069
20.414012	1105.610680	12.842074
20.619804	1108.402447	12.847079
20.432325	1110.159339	12.852083
20.190018	1104.102951	12.857088
20.294486	1106.891956	12.862093
20.517780	1101.589236	12.867098
20.085442	1112.028840	12.872103
20.230543	1109.750702	12.877107
20.606844	1105.975364	12.882112
20.360962	1110.247458	12.887117
20.392613	1106.687952	12.892122
20.431817	1106.423215	12.897127
20.221830	1105.436526	12.902131
20.277060	1114.051019	12.907136
20.125865	1107.503835	12.912141
20.608351	1106.190637	12.917146
20.379828	1112.410739	12.922151
20.344282	1111.181749	12.927155
20.309683	1110.972942	12.932160
20.165263	1111.355688	12.937165
20.346755	1107.978869	12.942170
20.176133	1116.127896	12.947175
20.364801	1109.247367	12.952179
20.537806	1105.220593	12.957184
20.144046	1114.933346	12.962189
20.335055	1110.648221	12.967194
20.151225	1116.701917	12.972199
20.173167	1113.113994	12.977203
20.591490	1109.535387	12.982208
20.290251	1115.393335	12.987213
20.503705	1110.260924	12.992218
20.200802	1122.324721	12.997223
20.335890	1114.337781	13.002227
20.561469	1114.171054	13.007232
20.133412	1113.211264	13.012237
20.262056	1111.303197	13.017242
20.093815	1115.845196	13.022247
20.176884	1114.210915	13.027251
20.164218	1109.019951	13.032256
20.191999	1122.377778	13.037261
20.359152	1117.391527	13.042266
20.146068	1117.414626	13.047271
20.513179	1118.964779	13.052275
20.491430	1117.709932	13.057280
20.514220	1121.434527	13.062285
20.792254	1105.656377	13.067290
20.403576	1115.037145	13.072295
20.420902	1120.901054	13.077299
20.523619	1122.658968	13.082304
20.502583	1121.552248	13.087309
20.537006	1124.846038	13.092314
19.885052	1122.917397	13.097319
20.154212	1119.354697	13.102323
20.426381	1122.285696	13.107328
20.412274	1125.420063	13.112333
20.684996	1111.547798	13.117338
20.261523	1129.434276	13.122343
20.151299	1119.762775	13.127347
20.476956	1122.713630	13.132352
20.449727	1122.393255	13.137357
20.276380	1111.334586	13.142362
20.088502	1112.468619	13.147367
20.494148	1113.358160	13.152371
20.454639	1119.360450	13.157376
20.231160	1120.394501	13.162381
20.137218	1110.617903	13.167386
20.018788	1125.661236	13.172391
20.388480	1120.844536	13.177395
20.290895	1130.096876	13.182400
20.315280	1130.178294	13.187405
20.149963	1132.745398	13.192410
20.058625	1131.304522	13.197415
20.433672	1133.112043	13.202419
20.098799	1137.120785	13.207424
20.085141	1130.975871	13.212429
20.449266	1137.050985	13.217434
20.316699	1132.983055	13.222439
20.416588	1134.113767	13.227443
20.285144	1123.431622	13.232448
20.359988	1135.488795	13.237453
20.364968	1134.265955	13.242458
20.472214	1143.900388	13.247463
20.391178	1137.903420	13.252467
20.663005	1127.844529	13.257472
20.162544	1133.420435	13.262477
20.163398	1135.992574	13.267482
20.346593	1139.861906	13.272487
20.265011	1134.691387	13.277491
20.379479	1143.209712	13.282496
20.213787	1137.748243	13.287501
20.603550	1135.681822	13.292506
20.321750	1137.879559	13.297511
20.307886	1135.732435	13.302515
20.192505	1141.243765	13.307520
20.341730	1149.911098	13.312525
20.486475	1134.660403	13.317530
20.387070	1128.248458	13.322535
20.379721	1110.087209	13.327539
20.310189	1105.083520	13.332544
20.105461	1105.956877	13.337549
20.271605	1118.464694	13.342554
20.119488	1124.368248	13.347559
20.642981	1130.930471	13.352563
20.414729	1108.491300	13.357568
20.021381	1108.983142	13.362573
20.471540	1109.977552	13.367578
20.058683	1115.465357	13.372583
20.108800	1120.772077	13.377587
20.501518	1144.934250	13.382592
20.335526	1146.067948	13.387597
20.339967	1135.835650	13.392602
20.250824	1144.580427	13.397607
20.195209	1144.281927	13.402611
20.454090	1136.642675	13.407616
20.317384	1144.988167	13.412621
20.393238	1132.178660	13.417626
20.655851	1136.079480	13.422631
20.431541	1121.177840	13.427635
20.327451	1110.809900	13.432640
20.124177	1103.337428	13.437645
20.117167	1096.947031	13.442650
20.360423	1114.209876	13.447655
20.311847	1119.212203	13.452659
20.515677	1111.466622	13.457664
19.965411	1120.042078	13.462669
20.088628	1120.216546	13.467674
20.375618	1126.483740	13.472679
20.385090	1144.247557	13.477683
20.488572	1152.215680	13.482688
20.055144	1127.461017	13.487693
20.546055	1128.120907	13.492698
20.370665	1125.070682	13.497703
19.914591	1124.804519	13.502707
20.182234	1121.082781	13.507712
20.132813	1154.386534	13.512717
20.203416	1143.393012	13.517722
20.295616	1161.085304	13.522727
20.418112	1154.983320	13.527731
20.618992	1151.707483	13.532736
20.373113	1154.747933	13.537741
20.590713	1144.562056	13.542746
20.158739	1134.798359	13.547751
20.165826	1126.699359	13.552755
20.563858	1132.983538	13.557760
20.345738	1133.267649	13.562765
20.357918	1123.590814	13.567770
20.548647	1114.817526	13.572775
20.748320	1109.685735	13.577779
20.481908	1111.903092	13.582784
20.200123	1115.307246	13.587789
20.588696	1106.447208	13.592794
20.403807	1121.474328	13.597799
20.316606	1111.308707	13.602803
20.690347	1107.727750	13.607808
20.407679	1112.467781	13.612813
20.622179	1121.717645	13.617818
20.559782	1128.010607	13.622823
20.453084	1111.767094	13.627827
20.720638	1109.411074	13.632832
20.137850	1097.255462	13.637837
20.625511	1089.328995	13.642842
20.270549	1095.525102	13.647847
20.259076	1094.667604	13.652851
20.572502	1078.076405	13.657856
20.235777	1087.346362	13.662861
20.285624	1082.008235	13.667866
20.414244	1086.277358	13.672871
20.763088	1074.976144	13.677875
20.054065	1091.963490	13.682880
20.043550	1088.426484	13.687885
20.541557	1089.388027	13.692890
20.652850	1084.292422	13.697895
20.371780	1096.437875	13.702899
20.448906	1086.615081	13.707904
20.241693	1082.653694	13.712909
20.449464	1082.447228	13.717914
20.612377	1087.570357	13.722919
20.485263	1082.610556	13.727923
20.671622	1071.860409	13.732928
20.308331	1086.991647	13.737933
20.460406	1097.481529	13.742938
20.265793	1087.940210	13.747943
20.616822	1081.924811	13.752947
20.444113	1061.303041	13.757952
20.073519	1058.025337	13.762957
20.316116	1059.090700	13.767962
20.091562	1074.037363	13.772967
19.921284	1077.980408	13.777971
20.087462	1083.068320	13.782976
19.813224	1097.146109	13.787981
20.268710	1082.699069	13.792986
20.173815	1091.559855	13.797991
20.182529	1093.277565	13.802995
19.953769	1086.346931	13.808000
20.101289	1091.456747	13.813005
20.563498	1090.160978	13.818010
20.416049	1096.360255	13.823015
20.270849	1091.783398	13.828019
20.573383	1084.324875	13.833024
19.972254	1091.362949	13.838029
20.253130	1097.068109	13.843034
19.962466	1094.274409	13.848039
20.097120	1089.400589	13.853043
20.173011	1096.185587	13.858048
20.392998	1094.665092	13.863053
20.503459	1101.884567	13.868058
20.247513	1102.983723	13.873063
20.260060	1097.664156	13.878067
20.440865	1092.872864	13.883072
20.305684	1102.591673	13.888077
20.326014	1098.989817	13.893082
20.333267	1106.605820	13.898087
20.396211	1091.249942	13.903091
20.233631	1097.040032	13.908096
20.215944	1098.227343	13.913101
20.285666	1084.884246	13.918106
20.066588	1103.813616	13.923111
20.215770	1090.438915	13.928115
20.222743	1096.022178	13.933120
20.170453	1125.074676	13.938125
20.334967	1117.945672	13.943130
20.459059	1132.761084	13.948135
20.234510	1128.047055	13.953139
20.314576	1114.997184	13.958144
20.352427	1125.379143	13.963149
20.712115	1128.351380	13.968154
20.416241	1117.484147	13.973159
20.405807	1105.226192	13.978163
20.700777	1103.088160	13.983168
19.963697	1111.004251	13.988173
20.389250	1105.065268	13.993178
20.301882	1107.435423	13.998183
20.439236	1100.927374	14.003187
20.376776	1099.945539	14.008192
20.154456	1107.537980	14.013210
20.722309	1101.205894	14.018227
20.073279	1101.054744	14.023245
20.289337	1096.070207	14.028263
20.324153	1102.309602	14.033280
20.199384	1101.659556	14.038298
20.198796	1108.864130	14.043315
20.013626	1106.625551	14.048333
20.201435	1126.067901	14.053351
20.221772	1130.969422	14.058368
20.563936	1140.725801	14.063386
20.633020	1133.021380	14.068403
20.799918	1131.470669	14.073421
20.473519	1123.930008	14.078439
20.503489	1132.611486	14.083456
20.562630	1131.395709	14.088474
20.716469	1142.281658	14.093491
20.613806	1135.087542	14.098509
20.685296	1137.212424	14.103527
20.755617	1137.434160	14.108544
20.552179	1145.721874	14.113562
20.939850	1139.207730	14.118579
20.563002	1138.275426	14.123597
20.497253	1140.079285	14.128615
21.036272	1135.785675	14.133632
20.664967	1144.831611	14.138650
21.018116	1134.270922	14.143667
20.801301	1142.000779	14.148685
20.850661	1139.679169	14.153703
20.624237	1122.767923	14.158720
20.725026	1133.177842	14.163738
20.944002	1126.225005	14.168755
20.750300	1139.362296	14.173773
20.615092	1139.827599	14.178791
20.895208	1137.017729	14.183808
20.855169	1140.292962	14.188826
20.799219	1138.274436	14.193843
20.473965	1149.825114	14.198861
20.568288	1141.855543	14.203879
20.741696	1137.791709	14.208896
20.463390	1150.486335	14.213914
20.608202	1159.124342	14.218931
21.044578	1169.468173	14.223949
20.913692	1173.184189	14.228967
21.112235	1165.339552	14.233984
21.083322	1181.159310	14.239002
21.140973	1177.301117	14.244019
21.227574	1172.458325	14.249037
21.097811	1180.597455	14.254055
21.508571	1175.853963	14.259072
21.355940	1184.339659	14.264090
21.249526	1173.027992	14.269107
21.202188	1182.461144	14.274125
21.146026	1186.890400	14.279143
21.508772	1176.491743	14.284160
21.489478	1180.186814	14.289178
21.351434	1191.072168	14.294195
21.381893	1186.762137	14.299213
20.922395	1179.974126	14.304231
21.266463	1179.497827	14.309248
20.968558	1181.459843	14.314266
21.108724	1179.985749	14.319283
21.462695	1179.207426	14.324301
21.361424	1180.928867	14.329319
21.686057	1175.599799	14.334336
21.364180	1184.480574	14.339354
21.400982	1179.136069	14.344371
21.533992	1176.253703	14.349389
21.140022	1180.436397	14.354407
21.321841	1183.229517	14.359424
21.199192	1191.616054	14.364442
21.642367	1206.363250	14.369459
22.140465	1204.050274	14.374477
21.697794	1202.389151	14.379495
21.662439	1182.641110	14.384512
21.569796	1190.890728	14.389530
21.418658	1194.665035	14.394547
21.373761	1200.399668	14.399565
21.881212	1203.515226	14.404583
21.953635	1209.128903	14.409600
21.715606	1211.021598	14.414618
22.075883	1219.066853	14.419635
22.155589	1220.995383	14.424653
21.656553	1216.530706	14.429671
21.882034	1193.599744	14.434688
21.991509	1206.776825	14.439706
21.749220	1199.199113	14.444723
21.841856	1201.136589	14.449741
21.997259	1198.629742	14.454759
21.896607	1215.338719	14.459776
21.930117	1212.531992	14.464794
21.965520	1216.657217	14.469811
21.989948	1214.135081	14.474829
21.751370	1224.210665	14.479847
21.919474	1213.484382	14.484864
21.980536	1222.835776	14.489882
21.961557	1215.027382	14.494899
21.740545	1214.414705	14.499917
21.575916	1217.801063	14.504935
21.891366	1214.136117	14.509952
22.064615	1221.341332	14.514970
21.664048	1215.915569	14.519987
22.015123	1241.578455	14.525005
21.950149	1248.332476	14.530023
22.195633	1245.320472	14.535040
22.083439	1250.115759	14.540058
22.330969	1246.455347	14.545075
22.566594	1248.582378	14.550093
22.344796	1250.382827	14.555111
22.595475	1249.303228	14.560128
22.137032	1251.935796	14.565146
22.386756	1243.725879	14.570163
22.721910	1244.510984	14.575181
22.341782	1252.216613	14.580199
22.635643	1238.387146	14.585216
22.503164	1240.838731	14.590234
22.383553	1249.520543	14.595251
22.557717	1245.539928	14.600269
22.442018	1243.394065	14.605287
22.722287	1241.583015	14.610304
22.573460	1249.202984	14.615322
22.614115	1250.272590	14.620339
22.916669	1239.199228	14.625357
22.337982	1232.905254	14.630375
22.121301	1230.629211	14.635392
22.214063	1245.852335	14.640410
22.230674	1257.625417	14.645427
22.468864	1243.616063	14.650445
22.323576	1245.874639	14.655463
22.842641	1241.198793	14.660480
22.859303	1244.318715	14.665498
22.725047	1243.336697	14.670515
22.827135	1235.855043	14.675533
22.432714	1241.939598	14.680551
22.676085	1247.032096	14.685568
22.661495	1244.824488	14.690586
22.701765	1264.853697	14.695603
22.958256	1263.543509	14.700621
22.567988	1274.360619	14.705639
23.281688	1271.253475	14.710656
23.150141	1268.617783	14.715674
23.117003	1268.786812	14.720691
23.044752	1259.613649	14.725709
23.145708	1257.522888	14.730727
23.135359	1242.765099	14.735744
23.126629	1242.703720	14.740762
23.168577	1241.814717	14.745779
23.031551	1236.453874	14.750797
23.156311	1241.173609	14.755815
23.011639	1235.148601	14.760832
23.455650	1236.386672	14.765850
22.760090	1245.460797	14.770867
23.201421	1255.659183	14.775885
23.532815	1259.694736	14.780903
23.475400	1248.869121	14.785920
23.388200	1251.319778	14.790938
23.115543	1246.872464	14.795955
23.565689	1240.041573	14.800973
23.373957	1257.539048	14.805991
23.506844	1245.045573	14.811008
23.563065	1250.707468	14.816026
23.503130	1246.149145	14.821043
23.528195	1254.913275	14.826061
23.354889	1244.493110	14.831079
23.284441	1241.163417	14.836096
23.344242	1248.751681	14.841114
23.301988	1256.606337	14.846131
23.401613	1249.183271	14.851149
23.050944	1256.352524	14.856167
22.905321	1250.543165	14.861184
23.155682	1264.646353	14.866202
23.317537	1267.066723	14.871219
23.522682	1265.149677	14.876237
23.277898	1271.149028	14.881255
23.227416	1258.393782	14.886272
23.678244	1265.230702	14.891290
23.537573	1262.942529	14.896307
23.596432	1258.481657	14.901325
23.792100	1273.375366	14.906343
23.829827	1270.305262	14.911360
23.896715	1263.478865	14.916378
23.557485	1270.466977	14.921395
24.039762	1278.659545	14.926413
23.890804	1277.900092	14.931431
23.698554	1276.581258	14.936448
23.786071	1292.403014	14.941466
23.869770	1291.958805	14.946483
23.993727	1302.797731	14.951501
23.975614	1312.053272	14.956519
24.291432	1290.688633	14.961536
24.544354	1277.639584	14.966554
24.111891	1276.425133	14.971571
24.421058	1266.363720	14.976589
24.192291	1275.042509	14.981607
24.033528	1269.538830	14.986624
24.214353	1267.718470	14.991642
23.899199	1273.754215	14.996659
24.370815	1278.500433	15.001677
24.291410	1276.490348	15.006695
24.188788	1264.328576	15.011712
24.530077	1270.527023	15.016730
24.006252	1279.106589	15.021747
24.231858	1279.267379	15.026765
24.453763	1264.209828	15.031783
24.482189	1266.656200	15.036800
24.458700	1274.257763	15.041818
24.343025	1278.197893	15.046835
24.481460	1265.876547	15.051853
24.493057	1277.895836	15.056871
24.128228	1283.239515	15.061888
24.119147	1269.010032	15.066906
24.213035	1276.404111	15.071923
24.300320	1276.653031	15.076941
24.372812	1268.686873	15.081959
24.289239	1274.216920	15.086976
24.546638	1266.634973	15.091994
24.291207	1269.161230	15.097011
24.593522	1281.731895	15.102029
24.268350	1271.092118	15.107047
24.320093	1294.564443	15.112064
24.920190	1303.111037	15.117082
24.761107	1301.764888	15.122099
24.731221	1297.006702	15.127117
24.910112	1290.768039	15.132135
24.713099	1280.737020	15.137152
24.762345	1276.140823	15.142170
24.374874	1279.035780	15.147187
24.799146	1288.138945	15.152205
24.910972	1296.532186	15.157223
24.529433	1306.366363	15.162240
24.708543	1309.595666	15.167258
24.854672	1312.569110	15.172275
24.736734	1304.011966	15.177293
24.691351	1310.482893	15.182311
24.474551	1310.830654	15.187328
24.539893	1311.248242	15.192346
24.630276	1321.504227	15.197363
24.733397	1306.335019	15.202381
24.786983	1311.088152	15.207399
25.076558	1322.136628	15.212416
25.251390	1326.950651	15.217434
25.230780	1336.313572	15.222451
25.034607	1325.009812	15.227469
25.362915	1311.675002	15.232487
25.197422	1313.916361	15.237504
25.502404	1312.647198	15.242522
25.202102	1312.102219	15.247539
25.216964	1300.797850	15.252557
25.320163	1312.462783	15.257575
25.338273	1318.289659	15.262592
25.016873	1303.156708	15.267610
25.149788	1315.125215	15.272627
25.426433	1315.139439	15.277645
25.411441	1330.691298	15.282663
25.365152	1332.408706	15.287680
25.642509	1335.019876	15.292698
25.228695	1307.995456	15.297715
25.479213	1318.192863	15.302733
25.648606	1334.923396	15.307751
25.402964	1328.739849	15.312768
25.865857	1327.108870	15.317786
25.495480	1318.801195	15.322803
25.277274	1312.701368	15.327821
25.434951	1323.906165	15.332839
25.736786	1328.632290	15.337856
26.022908	1327.764109	15.342874
25.949774	1328.502660	15.347891
25.688504	1312.919661	15.352909
25.748500	1298.160033	15.357927
25.599964	1306.560204	15.362944
25.547538	1294.299165	15.367962
25.651905	1318.895709	15.372979
25.807787	1334.045937	15.377997
25.478091	1324.130432	15.383015
25.887097	1329.415189	15.388032
25.967836	1323.657783	15.393050
25.955359	1345.200898	15.398067
26.024983	1333.005301	15.403085
26.055829	1326.886192	15.408103
25.819926	1337.798275	15.413120
26.214448	1323.376945	15.418138
25.992603	1333.814876	15.423155
26.128452	1333.989984	15.428173
25.878223	1333.529825	15.433191
25.874733	1330.430103	15.438208
25.960866	1331.199878	15.443226
25.935392	1333.231716	15.448243
26.018663	1332.213421	15.453261
26.487107	1328.300674	15.458279
26.248310	1331.344959	15.463296
26.254509	1330.716483	15.468314
26.283467	1333.584352	15.473331
26.041473	1331.672553	15.478349
26.296024	1324.735969	15.483367
26.209545	1328.540895	15.488384
26.458544	1338.592268	15.493402
25.914003	1331.995501	15.498419
26.069294	1327.214060	15.503437
26.112401	1329.469339	15.508455
25.741619	1336.475099	15.513472
26.345312	1355.508500	15.518490
26.382272	1353.602539	15.523507
26.238753	1362.974071	15.528525
26.776216	1358.624017	15.533543
26.606510	1367.244676	15.538560
26.794997	1357.496606	15.543578
26.875477	1369.283186	15.548595
26.782035	1367.711055	15.553613
27.121221	1346.477887	15.558631
26.539952	1331.818940	15.563648
26.520711	1329.306895	15.568666
26.655923	1335.347906	15.573683
26.743452	1347.479408	15.578701
26.947318	1353.635318	15.583719
26.830175	1352.446069	15.588736
27.017897	1342.632063	15.593754
26.691959	1329.469235	15.598771
26.540721	1338.285132	15.603789
26.782089	1337.848806	15.608807
26.712431	1368.847084	15.613824
26.957177	1364.516978	15.618842
26.878408	1365.215531	15.623859
26.977949	1365.273734	15.628877
27.189372	1367.330711	15.633895
26.922142	1360.773068	15.638912
26.951513	1367.914789	15.643930
27.296804	1359.483497	15.648947
27.097317	1364.221960	15.653965
27.163450	1353.642401	15.658983
27.116075	1363.129158	15.664000
26.823234	1362.299842	15.669018
27.101763	1360.688829	15.674035
27.127917	1369.029710	15.679053
27.143803	1362.299492	15.684071
27.286983	1359.944005	15.689088
27.255252	1356.754400	15.694106
27.576774	1356.160570	15.699123
27.359455	1364.639385	15.704141
27.439187	1356.731799	15.709159
27.329580	1363.725801	15.714176
27.009492	1352.723356	15.719194
27.341249	1354.998664	15.724211
27.259309	1367.852493	15.729229
27.493815	1352.086552	15.734247
27.178844	1366.409003	15.739264
27.422218	1361.707882	15.744282
27.728621	1369.321368	15.749299
27.390997	1383.661606	15.754317
27.734138	1373.589980	15.759335
27.813809	1381.702109	15.764352
27.620240	1379.922578	15.769370
27.882992	1380.167107	15.774387
27.889700	1372.640822	15.779405
27.852118	1368.516197	15.784423
27.774878	1358.321300	15.789440
27.645582	1365.744733	15.794458
27.808109	1350.002860	15.799475
27.453136	1371.028063	15.804493
27.907570	1372.423360	15.809511
27.925900	1376.691354	15.814528
27.825144	1391.102356	15.819546
27.775471	1382.018323	15.824563
27.810900	1387.332802	15.829581
27.877932	1382.741600	15.834599
27.791609	1383.859784	15.839616
27.888109	1375.049742	15.844634
28.092950	1380.955396	15.849651
27.854882	1390.241353	15.854669
27.955878	1386.870122	15.859687
27.831043	1382.633568	15.864704
27.997768	1387.483511	15.869722
27.889957	1390.530510	15.874739
28.127166	1407.424916	15.879757
28.552619	1406.179002	15.884775
28.516234	1417.392802	15.889792
28.566030	1404.613568	15.894810
28.407974	1375.976767	15.899827
28.263918	1392.285456	15.904845
28.408228	1375.969159	15.909863
28.250355	1382.583903	15.914880
28.530428	1401.915951	15.919898
29.016977	1386.512466	15.924915
28.837183	1392.035883	15.929933
28.843051	1371.082363	15.934951
28.618808	1379.021169	15.939968
28.382849	1385.111968	15.944986
28.593442	1376.176760	15.950003
28.706981	1381.980574	15.955021
28.503800	1373.935635	15.960039
28.463164	1375.661584	15.965056
28.290531	1376.463199	15.970074
28.672714	1384.423256	15.975091
28.642792	1367.466223	15.980109
28.913067	1375.916033	15.985127
28.848625	1376.958367	15.990144
28.736294	1370.926571	15.995162
28.831823	1374.614388	16.000179
28.545310	1388.693221	16.005197
28.806783	1400.679046	16.010215
28.957626	1401.418054	16.015232
29.114678	1409.900101	16.020250
29.073557	1409.911528	16.025267
29.246903	1405.957742	16.030285
29.159826	1389.838786	16.035303
28.678335	1391.830113	16.040320
28.915262	1387.101698	16.045338
29.102773	1414.365583	16.050355
29.020703	1409.038381	16.055373
29.223784	1405.361425	16.060391
29.468331	1406.241216	16.065408
29.253443	1409.805523	16.070426
29.240650	1397.523917	16.075443
29.136992	1412.654278	16.080461
29.000201	1408.153782	16.085479
29.398073	1411.947539	16.090496
29.313908	1407.344267	16.095514
29.298659	1415.934026	16.100531
29.048305	1413.205572	16.105549
29.504446	1407.122411	16.110567
29.646356	1403.019483	16.115584
29.260673	1406.859570	16.120602
29.753578	1407.556601	16.125619
29.579233	1407.274673	16.130637
29.527051	1403.216861	16.135655
29.532131	1406.733495	16.140672
29.452909	1415.468739	16.145690
29.788847	1402.840493	16.150707
29.470542	1407.505113	16.155725
29.286559	1408.349438	16.160743
29.600428	1396.080223	16.165760
29.391811	1408.520138	16.170778
29.845420	1424.653307	16.175795
29.680870	1438.931386	16.180813
29.709921	1435.533866	16.185831
29.915946	1445.774640	16.190848
29.791275	1440.060964	16.195866
29.931437	1430.031114	16.200883
29.957373	1442.378589	16.205901
29.955981	1438.550194	16.210919
30.328258	1430.897928	16.215936
30.073928	1437.864712	16.220954
30.008568	1432.945398	16.225971
29.757701	1440.792529	16.230989
30.302588	1428.889135	16.236007
30.315046	1431.029768	16.241024
30.366836	1440.958511	16.246042
30.339091	1425.602412	16.251059
29.772583	1427.761461	16.256077
30.034081	1432.361920	16.261095
30.114315	1426.146801	16.266112
30.149704	1433.973438	16.271130
30.187464	1432.079923	16.276147
29.944438	1436.622432	16.281165
30.249732	1436.122424	16.286183
30.174145	1435.673730	16.291200
30.085678	1436.361249	16.296218
30.567647	1435.255756	16.301235
30.164322	1429.069003	16.306253
30.340361	1441.864444	16.311271
30.736523	1460.507941	16.316288
30.525421	1466.909416	16.321306
30.746574	1455.455616	16.326323
30.784580	1444.614634	16.331341
30.814622	1438.490887	16.336359
30.958007	1438.279401	16.341376
30.406388	1435.027986	16.346394
30.711983	1424.273325	16.351411
30.199125	1438.251456	16.356429
30.804370	1453.739122	16.361447
31.050727	1456.781553	16.366464
30.679723	1459.202006	16.371482
30.944391	1459.002635	16.376499
31.069529	1465.613174	16.381517
31.195293	1456.571897	16.386535
31.353312	1452.567060	16.391552
30.922062	1453.158244	16.396570
31.058783	1436.091179	16.401587
31.321235	1434.350588	16.406605
31.125485	1432.192298	16.411623
31.066106	1412.084406	16.416640
30.941209	1431.213674	16.421658
31.076169	1438.868701	16.426675
31.147154	1454.020012	16.431693
31.439133	1457.772471	16.436711
31.246444	1458.325602	16.441728
30.930694	1460.339265	16.446746
31.431289	1454.294612	16.451763
31.357334	1458.722070	16.456781
31.465062	1453.731095	16.461799
31.748264	1451.180225	16.466816
31.298959	1457.072274	16.471834
31.716005	1451.427916	16.476851
31.958669	1449.040816	16.481869
31.473354	1437.207357	16.486887
31.542625	1416.976690	16.491904
31.454173	1413.964435	16.496922
31.556511	1415.916123	16.501939
31.550937	1417.197608	16.506957
31.484799	1447.761338	16.511975
31.797954	1440.258497	16.516992
31.640944	1445.559649	16.522010
31.540029	1454.081297	16.527027
31.355774	1455.333084	16.532045
31.575080	1449.130379	16.537063
32.223050	1440.323571	16.542080
31.840592	1460.094859	16.547098
31.813417	1452.451240	16.552115
32.089569	1450.782395	16.557133
32.029607	1452.385594	16.562151
31.979305	1450.378707	16.567168
31.759807	1449.894766	16.572186
32.133237	1441.729501	16.577203
31.755027	1456.288643	16.582221
31.448920	1449.815812	16.587239
32.043243	1447.555092	16.592256
31.493499	1453.706981	16.597274
31.839934	1457.037045	16.602291
32.407633	1474.290950	16.607309
32.198208	1478.148559	16.612327
32.261083	1471.283379	16.617344
32.403825	1481.850453	16.622362
32.536688	1476.757933	16.627379
32.624420	1481.238259	16.632397
32.354200	1464.492476	16.637415
32.645311	1462.212478	16.642432
32.202906	1458.871277	16.647450
32.493327	1462.537468	16.652467
32.716893	1468.260846	16.657485
32.612714	1454.773092	16.662503
32.769284	1446.840617	16.667520
32.704297	1448.705740	16.672538
32.430015	1449.141324	16.677555
32.485504	1446.115541	16.682573
32.695339	1466.517532	16.687591
32.971672	1470.703502	16.692608
32.839572	1460.314362	16.697626
32.866850	1458.376898	16.702643
32.862142	1441.195531	16.707661
32.766667	1445.148215	16.712679
32.959633	1443.329044	16.717696
32.657185	1452.134522	16.722714
33.079269	1449.890264	16.727731
33.271569	1463.782684	16.732749
32.789972	1452.434687	16.737767
33.048208	1446.059032	16.742784
32.802654	1461.775224	16.747802
32.974618	1468.497846	16.752819
33.350755	1467.261367	16.757837
32.946411	1465.056118	16.762855
32.923807	1472.539666	16.767872
32.928510	1466.827365	16.772890
33.039696	1471.300801	16.777907
33.193344	1455.544500	16.782925
32.967288	1468.669945	16.787943
32.954536	1463.676161	16.792960
32.975128	1460.843132	16.797978
33.113601	1471.755376	16.802995
33.042915	1481.028849	16.808013
33.286990	1494.886298	16.813031
33.445316	1502.671340	16.818048
33.467411	1492.660280	16.823066
33.478471	1501.820053	16.828083
33.514045	1509.366700	16.833101
33.345494	1506.423831	16.838119
33.644821	1491.698192	16.843136
33.277482	1511.835230	16.848154
33.513066	1510.377344	16.853171
33.725995	1497.916503	16.858189
33.704135	1509.172103	16.863207
33.567333	1501.004819	16.868224
33.645918	1499.741865	16.873242
33.321160	1511.719042	16.878259
33.704518	1520.371126	16.883277
33.753749	1521.928600	16.888295
34.024278	1527.559566	16.893312
34.477092	1522.867460	16.898330
34.231679	1528.563418	16.903347
34.341773	1516.315595	16.908365
33.965664	1514.206509	16.913383
33.993729	1498.825700	16.918400
33.882733	1512.816881	16.923418
33.932948	1516.559154	16.928435
34.257440	1527.416599	16.933453
33.718182	1537.269795	16.938471
34.322455	1524.850331	16.943488
34.301084	1534.139567	16.948506
34.463990	1541.113782	16.953523
34.816837	1517.587832	16.958541
34.723037	1526.352209	16.963559
34.807942	1517.963933	16.968576
34.681406	1523.645647	16.973594
34.595650	1494.493705	16.978611
34.529300	1486.170472	16.983629
34.279244	1486.649384	16.988647
34.608899	1490.910225	16.993664
34.334558	1503.681605	16.998682
34.506811	1513.646240	17.003699
34.775275	1522.407888	17.008717
34.954548	1513.161411	17.013735
34.860549	1521.000868	17.018752
34.795783	1524.980135	17.023770
34.944768	1512.615998	17.028787
34.745139	1517.552736	17.033805
34.974273	1516.070710	17.038823
35.099007	1498.794696	17.043840
34.859506	1495.531234	17.048858
34.750177	1508.221241	17.053875
35.098225	1509.120710	17.058893
35.138341	1509.786149	17.063911
35.097191	1506.162281	17.068928
34.977615	1503.748008	17.073946
34.809460	1508.778824	17.078963
35.039875	1499.230039	17.083981
34.828318	1521.012811	17.088999
35.047221	1519.106122	17.094016
34.878954	1508.378220	17.099034
34.936867	1511.483754	17.104051
34.901661	1506.205671	17.109069
35.275541	1510.846433	17.114087
35.150478	1519.195790	17.119104
35.480732	1531.129854	17.124122
35.594748	1539.895699	17.129139
35.777463	1521.759391	17.134157
35.526859	1516.938810	17.139175
35.538047	1512.427261	17.144192
35.772878	1508.441618	17.149210
35.606912	1517.505367	17.154227
35.459840	1510.193878	17.159245
35.378644	1512.111932	17.164263
35.539852	1533.912344	17.169280
35.454850	1537.921585	17.174298
35.427118	1538.472004	17.179315
35.903284	1540.060483	17.184333
35.602988	1550.496925	17.189351
35.814312	1549.047625	17.194368
35.880058	1553.762719	17.199386
35.628168	1549.665933	17.204403
35.825196	1545.373273	17.209421
36.145318	1551.833199	17.214439
35.653910	1545.533028	17.219456
35.887841	1552.712999	17.224474
35.917830	1554.020285	17.229491
36.101064	1553.476821	17.234509
36.310774	1575.302593	17.239527
36.344234	1565.225176	17.244544
36.776690	1563.210486	17.249562
36.573615	1558.662312	17.254579
36.607005	1552.366520	17.259597
36.452362	1546.722076	17.264615
36.647645	1542.624753	17.269632
36.437812	1542.189604	17.274650
36.307865	1544.459935	17.279667
36.647887	1534.247123	17.284685
36.457376	1546.191904	17.289703
36.492898	1540.342522	17.294720
36.608819	1543.772297	17.299738
36.167405	1542.584417	17.304755
36.607086	1538.197998	17.309773
36.045721	1537.424086	17.314791
36.544778	1558.242550	17.319808
37.012828	1563.558876	17.324826
36.903469	1578.742230	17.329843
36.799274	1567.722487	17.334861
36.525608	1585.590508	17.339879
36.871965	1571.906511	17.344896
36.952231	1575.450520	17.349914
36.462295	1566.914802	17.354931
36.825063	1566.345847	17.359949
36.885581	1565.505773	17.364967
36.866316	1567.928343	17.369984
37.278266	1565.130399	17.375002
36.753845	1575.763059	17.380019
37.029896	1560.784656	17.385037
37.038163	1572.952587	17.390055
37.060854	1564.489262	17.395072
37.262939	1575.817734	17.400090
37.231339	1569.974328	17.405107
37.347918	1569.959028	17.410125
37.469893	1565.442376	17.415143
37.256784	1577.318427	17.420160
37.244521	1582.610697	17.425178
37.224756	1595.593239	17.430195
37.584882	1592.904231	17.435213
37.363213	1604.273574	17.440231
37.657493	1600.884048	17.445248
37.670553	1608.239279	17.450266
37.490336	1603.360250	17.455283
37.735858	1605.235641	17.460301
37.611512	1601.467714	17.465319
37.748027	1606.777162	17.470336
37.777637	1603.758620	17.475354
37.794292	1609.342021	17.480371
37.850295	1596.965902	17.485389
38.051761	1598.206515	17.490407
37.773509	1599.739153	17.495424
37.909699	1593.288518	17.500442
37.785160	1599.614894	17.505459
38.032684	1598.458695	17.510477
37.971745	1599.086773	17.515495
37.891953	1600.101683	17.520512
38.053446	1595.745462	17.525530
38.108284	1604.736293	17.530547
37.850584	1591.057391	17.535565
37.967420	1610.256878	17.540583
38.105024	1616.366839	17.545600
38.509080	1619.409321	17.550618
38.330125	1634.669902	17.555635
38.464051	1619.399497	17.560653
38.587548	1630.956055	17.565671
38.390785	1630.315894	17.570688
38.738133	1623.713586	17.575706
38.527291	1626.026721	17.580723
38.927024	1624.594553	17.585741
38.759248	1615.565392	17.590759
38.460918	1605.860197	17.595776
38.594420	1615.735128	17.600794
38.641853	1616.342775	17.605811
38.744768	1611.302176	17.610829
38.751665	1613.292710	17.615847
38.579336	1612.387525	17.620864
39.078734	1614.326246	17.625882
38.716221	1622.227462	17.630899
38.887556	1612.761961	17.635917
39.118589	1620.666033	17.640935
38.742523	1609.895693	17.645952
39.086378	1622.063621	17.650970
38.879674	1620.556720	17.655987
38.919945	1617.313101	17.661005
38.975389	1620.486694	17.666023
38.876622	1613.493070	17.671040
39.253533	1617.235170	17.676058
39.034539	1622.096378	17.681075
39.083475	1611.851289	17.686093
39.384389	1611.894678	17.691111
39.495808	1619.698277	17.696128
39.166379	1606.875531	17.701146
39.476038	1618.174293	17.706163
39.593370	1618.243818	17.711181
39.386487	1609.656633	17.716199
39.352970	1621.420702	17.721216
39.892809	1624.575237	17.726234
39.462030	1636.662237	17.731251
39.900716	1637.476471	17.736269
39.805130	1621.986263	17.741287
39.632160	1620.824773	17.746304
39.806233	1626.817235	17.751322
39.987450	1634.238468	17.756339
39.707666	1618.483483	17.761357
39.769382	1635.432890	17.766375
39.443438	1639.383060	17.771392
39.836745	1629.312696	17.776410
39.327475	1656.181652	17.781427
39.394884	1642.450845	17.786445
39.683432	1646.527951	17.791463
39.585017	1646.351884	17.796480
40.026829	1663.258001	17.801498
40.173633	1655.432365	17.806515
40.168428	1663.507852	17.811533
40.277524	1656.454310	17.816551
40.278291	1662.831515	17.821568
40.462494	1653.477194	17.826586
40.455466	1652.061139	17.831603
40.732901	1657.050821	17.836621
40.955951	1652.551055	17.841639
40.652483	1657.974746	17.846656
40.737508	1656.762663	17.851674
40.566866	1648.396195	17.856691
40.399423	1648.660583	17.861709
40.691839	1641.980511	17.866727
40.737086	1655.703084	17.871744
40.908872	1649.235736	17.876762
40.936590	1656.436067	17.881779
40.530800	1640.457332	17.886797
40.946476	1643.059083	17.891815
40.652128	1648.141535	17.896832
41.166117	1643.911551	17.901850
40.894332	1636.862140	17.906867
40.578576	1637.623674	17.911885
40.403278	1638.763934	17.916903
40.331154	1642.860813	17.921920
40.813963	1630.735919	17.926938
40.580938	1643.374986	17.931955
40.668632	1652.821511	17.936973
40.996218	1668.817750	17.941991
40.881412	1662.844430	17.947008
41.192147	1672.518093	17.952026
41.322658	1666.099793	17.957043
41.197504	1667.227338	17.962061
41.230200	1661.985559	17.967079
41.312586	1667.221864	17.972096
41.635292	1664.886459	17.977114
41.344393	1664.741094	17.982131
41.396040	1662.640837	17.987149
41.517280	1654.342643	17.992167
41.422813	1669.010898	17.997184
41.819223	1660.374649	18.002202
41.577445	1667.894829	18.007219
41.747921	1685.467182	18.012237
41.877759	1682.520728	18.017255
41.772644	1688.817303	18.022272
42.249094	1683.885417	18.027290
42.061754	1665.284126	18.032307
41.836584	1667.244041	18.037325
41.983289	1657.120182	18.042343
41.978528	1671.873235	18.047360
42.435112	1674.987576	18.052378
42.670144	1670.715560	18.057395
42.457848	1660.519969	18.062413
42.748070	1647.367111	18.067431
41.946446	1646.683423	18.072448
42.382704	1645.061381	18.077466
42.064392	1647.240647	18.082483
41.926872	1638.922385	18.087501
42.154832	1645.364020	18.092519
42.137233	1645.261581	18.097536
42.330899	1665.682164	18.102554
42.584109	1671.850790	18.107571
42.506499	1684.257459	18.112589
42.551162	1674.360653	18.117607
42.241313	1680.870782	18.122624
42.498107	1674.256153	18.127642
42.895848	1681.987375	18.132659
42.464524	1675.281150	18.137677
42.650159	1673.562223	18.142695
42.142425	1680.934490	18.147712
42.260899	1673.152691	18.152730
42.786256	1686.015331	18.157747
42.576495	1702.610133	18.162765
42.912620	1699.550546	18.167783
42.706508	1713.066296	18.172800
43.144580	1709.924377	18.177818
43.401681	1706.525028	18.182835
43.119280	1713.101580	18.187853
43.301403	1699.552201	18.192871
43.325441	1711.104238	18.197888
43.415272	1706.289069	18.202906
43.370061	1705.138654	18.207923
43.290116	1714.956460	18.212941
43.631210	1690.892545	18.217959
43.714477	1708.274338	18.222976
43.580536	1698.207798	18.227994
43.836128	1698.319766	18.233011
43.544755	1679.280436	18.238029
43.666528	1667.727488	18.243047
43.456530	1667.525173	18.248064
43.570121	1679.394816	18.253082
43.729047	1678.938597	18.258099
43.456610	1710.852437	18.263117
43.908130	1688.564205	18.268135
43.637630	1701.613576	18.273152
43.761325	1700.626562	18.278170
43.546990	1695.966879	18.283187
43.695221	1697.011494	18.288205
43.898757	1697.580088	18.293223
43.683771	1704.933989	18.298240
44.094299	1703.097389	18.303258
43.928647	1703.092498	18.308275
43.679061	1712.635332	18.313293
43.850532	1711.551032	18.318311
44.119247	1727.314475	18.323328
44.079966	1729.430370	18.328346
44.394241	1723.950169	18.333363
44.267672	1733.342831	18.338381
44.687738	1726.859443	18.343399
44.341148	1726.540484	18.348416
44.760769	1723.182850	18.353434
44.766569	1723.160051	18.358451
44.498238	1716.990966	18.363469
44.709888	1717.520514	18.368487
44.518853	1719.215435	18.373504
44.544599	1733.081195	18.378522
45.101757	1714.928969	18.383539
44.823044	1717.138109	18.388557
44.829876	1724.129442	18.393575
44.864290	1717.509363	18.398592
44.805848	1719.250778	18.403610
44.834386	1719.084349	18.408627
44.506521	1723.476879	18.413645
44.696577	1719.965521	18.418663
45.036944	1732.541523	18.423680
45.114955	1735.834241	18.428698
45.375491	1745.615065	18.433715
45.214715	1754.148009	18.438733
45.331515	1744.005263	18.443751
45.533881	1732.872002	18.448768
45.178589	1718.777524	18.453786
45.158193	1714.335446	18.458803
45.091878	1741.484700	18.463821
45.774522	1731.701607	18.468839
45.484374	1741.431833	18.473856
45.557261	1745.137514	18.478874
45.855500	1733.326700	18.483891
45.615421	1746.838459	18.488909
45.759075	1746.244672	18.493927
45.782892	1740.979112	18.498944
45.781738	1738.014213	18.503962
45.818464	1732.793789	18.508979
45.738566	1751.114037	18.513997
45.940979	1739.911548	18.519015
45.878426	1744.205136	18.524032
45.662167	1751.032285	18.529050
45.909183	1748.216569	18.534067
45.403271	1741.781766	18.539085
46.111063	1736.784649	18.544103
45.766499	1744.417220	18.549120
45.556683	1750.060394	18.554138
46.185242	1759.738481	18.559155
45.972532	1780.791921	18.564173
46.054354	1774.636177	18.569191
46.376756	1775.228288	18.574208
46.383384	1776.400891	18.579226
46.685178	1778.811613	18.584243
46.472750	1774.931844	18.589261
46.063905	1779.483602	18.594279
46.340102	1770.440160	18.599296
46.326584	1775.180553	18.604314
46.555847	1777.209576	18.609331
46.640516	1797.372442	18.614349
46.465392	1805.587584	18.619367
47.099009	1797.806139	18.624384
46.693617	1811.828046	18.629402
47.062316	1808.442335	18.634419
47.167627	1803.455559	18.639437
47.296795	1801.533260	18.644455
47.204428	1811.789640	18.649472
47.166251	1811.006981	18.654490
47.381450	1814.741893	18.659507
47.156389	1795.691832	18.664525
47.703067	1800.787276	18.669543
47.416620	1776.721849	18.674560
47.381928	1781.687424	18.679578
47.503175	1767.258907	18.684595
47.401195	1774.926736	18.689613
47.625074	1771.636493	18.694631
47.620198	1773.086217	18.699648
47.530993	1767.524060	18.704666
47.725483	1764.652224	18.709683
47.417560	1770.676006	18.714701
47.551692	1767.357606	18.719719
47.619711	1769.863818	18.724736
47.498888	1774.221766	18.729754
47.546338	1773.583545	18.734771
47.583531	1794.613663	18.739789
47.782850	1796.679713	18.744807
47.759754	1803.678216	18.749824
48.103410	1800.255601	18.754842
48.156826	1791.803761	18.759859
48.047195	1798.809773	18.764877
48.122408	1802.668472	18.769895
48.046468	1797.837240	18.774912
48.056507	1804.870573	18.779930
48.075789	1790.547175	18.784947
48.034659	1795.463443	18.789965
48.071095	1799.260685	18.794983
48.260829	1798.694940	18.800000
47.904602	1805.611294	18.805018
48.487005	1827.650145	18.810035
48.323537	1821.878009	18.815053
48.574015	1830.977779	18.820071
48.659369	1836.625818	18.825088
48.511218	1833.377597	18.830106
48.598506	1837.320112	18.835123
48.912660	1835.715167	18.840141
49.105998	1818.663005	18.845159
48.840992	1834.400791	18.850176
48.781770	1839.772220	18.855194
49.121732	1830.923070	18.860211
48.968933	1838.390605	18.865229
49.000271	1833.982712	18.870247
49.084512	1827.840717	18.875264
48.809210	1832.220176	18.880282
49.270327	1829.727385	18.885299
49.375266	1832.659528	18.890317
49.131438	1832.236083	18.895335
49.110119	1830.417223	18.900352
49.123564	1835.966616	18.905370
49.336173	1827.701729	18.910387
49.061523	1828.641551	18.915405
48.896050	1836.933826	18.920423
49.422030	1852.569852	18.925440
49.313947	1864.579613	18.930458
49.440324	1864.438478	18.935475
49.754638	1871.170045	18.940493
49.611679	1857.601581	18.945511
49.732448	1859.830398	18.950528
49.683423	1868.132433	18.955546
49.964371	1858.026349	18.960563
49.944462	1865.098309	18.965581
49.983025	1852.194626	18.970599
50.230660	1857.030250	18.975616
50.319516	1862.275819	18.980634
50.545652	1854.348544	18.985651
50.463310	1854.314634	18.990669
50.441055	1853.912478	18.995687
50.478807	1858.167292	19.000704
50.256686	1859.161661	19.005722
50.514411	1852.385563	19.010739
50.483851	1855.989791	19.015757
50.344256	1845.901240	19.020775
50.716421	1847.081615	19.025792
50.484068	1855.000736	19.030810
50.667558	1846.745989	19.035827
50.862937	1851.112516	19.040845
50.456317	1851.048528	19.045863
50.856402	1840.560073	19.050880
50.482702	1845.756713	19.055898
50.724614	1843.335064	19.060915
50.726573	1840.555271	19.065933
50.525825	1848.377323	19.070951
50.925222	1848.732207	19.075968
50.273844	1850.689337	19.080986
50.311580	1858.644035	19.086003
50.494855	1872.771103	19.091021
50.414799	1872.949194	19.096039
50.919568	1877.846063	19.101056
50.550698	1891.653788	19.106074
51.199309	1904.069873	19.111091
51.354174	1909.781575	19.116109
51.105643	1914.028582	19.121127
51.539352	1915.089817	19.126144
51.531902	1913.086256	19.131162
51.811664	1904.784659	19.136179
51.623586	1904.434119	19.141197
51.626039	1911.932773	19.146215
51.884802	1901.137255	19.151232
51.601303	1905.675351	19.156250
51.795669	1907.903449	19.161267
52.101345	1906.901553	19.166285
52.044385	1908.843322	19.171303
51.971064	1911.067710	19.176320
52.200115	1912.207207	19.181338
52.159579	1924.799297	19.186355
52.086618	1914.224999	19.191373
52.134412	1911.843738	19.196391
52.435886	1908.631541	19.201408
51.830684	1914.133340	19.206426
52.263771	1908.789070	19.211443
52.068555	1900.871558	19.216461
52.047323	1911.174081	19.221479
51.977938	1900.082463	19.226496
52.483925	1911.719817	19.231514
52.321358	1908.250500	19.236531
52.418095	1918.711183	19.241549
52.289612	1919.965911	19.246567
52.788215	1904.806149	19.251584
52.363821	1929.213562	19.256602
52.561133	1913.500140	19.261619
52.464995	1913.534500	19.266637
52.217306	1931.207669	19.271655
52.563852	1940.577702	19.276672
52.654183	1941.140767	19.281690
52.828285	1950.791578	19.286707
52.933271	1940.177866	19.291725
52.934056	1937.950397	19.296743
53.312657	1937.968814	19.301760
53.050846	1942.725267	19.306778
53.092768	1945.564448	19.311795
53.556671	1948.676111	19.316813
53.268335	1967.889570	19.321831
53.636591	1966.426212	19.326848
53.673053	1954.257408	19.331866
53.658566	1953.113871	19.336883
53.683078	1943.120206	19.341901
53.487926	1940.005303	19.346919
53.957638	1937.992489	19.351936
53.542603	1944.537601	19.356954
53.656219	1953.932996	19.361971
53.964977	1949.494192	19.366989
54.034099	1969.939001	19.372007
54.227274	1961.722758	19.377024
54.239454	1952.033873	19.382042
53.980667	1943.627807	19.387059
54.309264	1949.567443	19.392077
54.326955	1945.008317	19.397095
54.383084	1931.222405	19.402112
54.293509	1936.016668	19.407130
54.226406	1939.846979	19.412147
54.587610	1920.889656	19.417165
54.208663	1936.471112	19.422183
54.479079	1946.014533	19.427200
54.511073	1943.064756	19.432218
54.446601	1953.936584	19.437235
54.553574	1956.243912	19.442253
54.520216	1954.283805	19.447271
54.462726	1949.675318	19.452288
54.688020	1947.935877	19.457306
54.655957	1948.914882	19.462323
54.883399	1939.020992	19.467341
54.666085	1949.875509	19.472359
54.730819	1947.559970	19.477376
54.831276	1963.416577	19.482394
54.936949	1965.244320	19.487411
55.403622	1975.196924	19.492429
55.342676	1978.273537	19.497447
55.451418	1980.353275	19.502464
55.621294	1985.384610	19.507482
55.571226	1974.431433	19.512499
55.671295	1954.115666	19.517517
55.242220	1946.388805	19.522535
55.252903	1957.348540	19.527552
55.473987	1959.539349	19.532570
55.380382	1977.790493	19.537587
56.049990	1963.331738	19.542605
55.483922	1979.360740	19.547623
56.079079	1963.747411	19.552640
55.379718	1974.646582	19.557658
55.395418	1975.554261	19.562675
55.830704	1977.923276	19.567693
55.735477	1970.446762	19.572711
55.594477	1969.829938	19.577728
55.882022	1979.156708	19.582746
55.622437	1982.984695	19.587763
56.057712	1986.597244	19.592781
56.044412	1994.682858	19.597799
56.353865	1996.550465	19.602816
56.037427	1987.260838	19.607834
55.923469	1992.235982	19.612851
56.333628	1987.338954	19.617869
56.363513	1990.036124	19.622887
56.177008	2000.772502	19.627904
56.694241	2007.649528	19.632922
56.365932	2008.991980	19.637939
56.899080	2015.039023	19.642957
56.377169	2025.428562	19.647975
56.768283	2023.657158	19.652992
56.968505	2023.149510	19.658010
56.782741	2019.281939	19.663027
56.783290	2013.736834	19.668045
56.690460	2016.106715	19.673063
56.910904	2022.947711	19.678080
57.199197	2043.400927	19.683098
57.157575	2047.832844	19.688115
57.323629	2048.855766	19.693133
57.193469	2040.389801	19.698151
57.352170	2036.622234	19.703168
57.165866	2049.501963	19.708186
57.197490	2044.664504	19.713203
57.693207	2037.581363	19.718221
57.790445	2036.261116	19.723239
57.670505	2035.592164	19.728256
57.809367	2028.799549	19.733274
57.845984	2037.228026	19.738291
57.921612	2029.438713	19.743309
57.857817	2044.183469	19.748327
57.943411	2033.548399	19.753344
57.924909	2039.711755	19.758362
57.760396	2028.152271	19.763379
57.926639	2044.819631	19.768397
57.893781	2051.903185	19.773415
58.302833	2070.749920	19.778432
58.317731	2066.746507	19.783450
58.356576	2059.545092	19.788467
58.696536	2053.186029	19.793485
58.572487	2070.996171	19.798503
58.696191	2058.987192	19.803520
58.672689	2055.571167	19.808538
58.437277	2061.977565	19.813555
58.793990	2049.842549	19.818573
58.687163	2052.585919	19.823591
58.555265	2057.779461	19.828608
58.583147	2058.611267	19.833626
58.451719	2053.290126	19.838643
58.822488	2049.267712	19.843661
58.634916	2060.388140	19.848679
58.625075	2055.880563	19.853696
59.034250	2053.713001	19.858714
59.223370	2079.836598	19.863731
59.401471	2080.991314	19.868749
59.163051	2085.825884	19.873767
59.588756	2078.221394	19.878784
59.732754	2079.580548	19.883802
59.763360	2073.835561	19.888819
59.700157	2046.018410	19.893837
59.544808	2051.205465	19.898855
59.510377	2041.064610	19.903872
59.449599	2053.689143	19.908890
59.389156	2073.156630	19.913907
59.680069	2074.943045	19.918925
60.163778	2066.462529	19.923943
59.973923	2057.757525	19.928960
59.757148	2065.332911	19.933978
59.864989	2065.105851	19.938995
59.944438	2066.232254	19.944013
59.663544	2066.797901	19.949031
59.660981	2070.868074	19.954048
59.908047	2076.593454	19.959066
60.268262	2092.244382	19.964083
60.351193	2091.772743	19.969101
60.044698	2101.715824	19.974119
60.305238	2102.958073	19.979136
60.526119	2100.567266	19.984154
60.469895	2101.389678	19.989171
60.581219	2104.463224	19.994189
60.465162	2105.260571	19.999207
60.646429	2116.324573	20.004224
60.671024	2116.010897	20.009242
60.525000	2134.025979	20.014259
60.889379	2120.087686	20.019277
61.149188	2129.792590	20.024295
60.958291	2126.340323	20.029312
61.177745	2122.437196	20.034330
60.975957	2130.585197	20.039347
61.226218	2122.895403	20.044365
61.212536	2118.080090	20.049383
61.167058	2112.422732	20.054400
61.179118	2122.522669	20.059418
61.296994	2134.052210	20.064435
61.780029	2146.209396	20.069453
61.930483	2146.367242	20.074471
62.082566	2153.861820	20.079488
62.218841	2126.486993	20.084506
61.885814	2130.056156	20.089523
62.032052	2112.094828	20.094541
62.037531	2108.882605	20.099559
61.966481	2115.011113	20.104576
62.284791	2110.833447	20.109594
61.907422	2105.609718	20.114611
62.127193	2114.709060	20.119629
62.032676	2114.727430	20.124647
62.274335	2111.495628	20.129664
62.181023	2112.139902	20.134682
61.946203	2118.866357	20.139699
62.405924	2123.459808	20.144717
62.468320	2134.495590	20.149735
62.253817	2154.553290	20.154752
62.579262	2133.438368	20.159770
62.308382	2142.105509	20.164787
62.445594	2154.976206	20.169805
62.500420	2141.944610	20.174823
62.550064	2140.440813	20.179840
62.441559	2142.045536	20.184858
62.463607	2156.620976	20.189875
62.801061	2171.230287	20.194893
63.197909	2160.799540	20.199911
62.841242	2171.998935	20.204928
63.077708	2163.156654	20.209946
63.073330	2168.753851	20.214963
62.924309	2176.600862	20.219981
62.981078	2179.006687	20.224999
63.400585	2197.969118	20.230016
63.916396	2204.593195	20.235034
63.752618	2209.063522	20.240051
64.174743	2195.878122	20.245069
64.041318	2196.023041	20.250087
63.973219	2189.101330	20.255104
64.148060	2170.694895	20.260122
63.426713	2157.245929	20.265139
63.881849	2182.274085	20.270157
64.019614	2186.957448	20.275175
63.786208	2193.986536	20.280192
64.176817	2193.012764	20.285210
63.974185	2190.177441	20.290227
63.964094	2200.753687	20.295245
64.567368	2194.956643	20.300263
64.332354	2199.518558	20.305280
64.455578	2178.440543	20.310298
64.501088	2178.300505	20.315315
64.462658	2185.245792	20.320333
64.547733	2185.205629	20.325351
64.605629	2192.033304	20.330368
64.547727	2183.139641	20.335386
64.417834	2207.345595	20.340403
64.759414	2219.388543	20.345421
64.954279	2212.310828	20.350439
64.877929	2230.143446	20.355456
64.992012	2216.788494	20.360474
64.840392	2215.090261	20.365491
65.046998	2220.859905	20.370509
65.093646	2214.094497	20.375527
65.211225	2213.825767	20.380544
65.286563	2206.480024	20.385562
65.201813	2202.726074	20.390579
65.110383	2215.221921	20.395597
65.616797	2222.612828	20.400615
65.583337	2242.861225	20.405632
65.487585	2232.493262	20.410650
66.069240	2233.727568	20.415667
65.970525	2230.298327	20.420685
66.243682	2238.177144	20.425703
66.187982	2230.847570	20.430720
66.245344	2228.682609	20.435738
65.740999	2225.880455	20.440755
65.787801	2225.008710	20.445773
66.420360	2218.969446	20.450791
66.037117	2225.079362	20.455808
66.341449	2223.711912	20.460826
66.349093	2228.249291	20.465843
66.397259	2226.537283	20.470861
66.658505	2214.473203	20.475879
66.245365	2231.566687	20.480896
66.803305	2227.072326	20.485914
66.569774	2233.057688	20.490931
66.732162	2223.720641	20.495949
66.734670	2221.333968	20.500967
66.728537	2230.814714	20.505984
66.665305	2234.897756	20.511002
66.960410	2246.287428	20.516019
67.038878	2250.133930	20.521037
66.976951	2242.434872	20.526055
66.852641	2248.373718	20.531072
67.302142	2252.547245	20.536090
66.932557	2247.761910	20.541107
66.837077	2259.038484	20.546125
67.394455	2250.496561	20.551143
67.300014	2278.581018	20.556160
67.320842	2275.397773	20.561178
67.406385	2284.454919	20.566195
67.770233	2284.830433	20.571213
67.876901	2282.713446	20.576231
67.719618	2284.688570	20.581248
67.752980	2284.573279	20.586266
68.110225	2276.572167	20.591283
67.779690	2284.921697	20.596301
68.149017	2284.348528	20.601319
68.096935	2305.850618	20.606336
68.074412	2304.624173	20.611354
68.252737	2301.781554	20.616371
68.266639	2305.415771	20.621389
68.403920	2301.034887	20.626407
67.924190	2301.366396	20.631424
68.694910	2294.343885	20.636442
68.693292	2298.209465	20.641459
68.420613	2301.003717	20.646477
68.850749	2289.183218	20.651495
69.196933	2294.267558	20.656512
68.830102	2296.331163	20.661530
68.749651	2308.119791	20.666547
68.673384	2314.793518	20.671565
69.132390	2325.408302	20.676583
69.295877	2334.020437	20.681600
69.526367	2334.250470	20.686618
69.502760	2329.765455	20.691635
69.422763	2323.707652	20.696653
69.662310	2315.117276	20.701671
69.640758	2325.901520	20.706688
69.623736	2313.889606	20.711706
69.474741	2313.108076	20.716723
69.421222	2318.403262	20.721741
69.926294	2318.049131	20.726759
69.673613	2332.208424	20.731776
69.715468	2313.098594	20.736794
69.448843	2325.100198	20.741811
69.418191	2325.160295	20.746829
69.998142	2321.649535	20.751847
70.255768	2339.592627	20.756864
70.222810	2337.019669	20.761882
70.149406	2343.031450	20.766899
70.095295	2334.517788	20.771917
70.516528	2344.772072	20.776935
70.142320	2344.527502	20.781952
70.072593	2341.291040	20.786970
70.631611	2342.539980	20.791987
70.403931	2369.063291	20.797005
70.859257	2368.105144	20.802023
70.841299	2364.863567	20.807040
70.560385	2365.422934	20.812058
70.853085	2363.314807	20.817075
71.134006	2365.571647	20.822093
71.095186	2354.723363	20.827111
71.151227	2361.914807	20.832128
71.127374	2372.507530	20.837146
71.491034	2358.475524	20.842163
70.954998	2373.022992	20.847181
71.395889	2390.262042	20.852199
71.539747	2397.980657	20.857216
71.659199	2402.235971	20.862234
71.884515	2393.154640	20.867251
71.860334	2391.989018	20.872269
72.007676	2389.526518	20.877287
71.798464	2394.192137	20.882304
71.768618	2390.580403	20.887322
72.179438	2379.854669	20.892339
72.048414	2386.154102	20.897357
72.407165	2386.918211	20.902375
72.049659	2388.320411	20.907392
71.837606	2376.455176	20.912410
72.414707	2382.181527	20.917427
72.476362	2396.800445	20.922445
72.451819	2387.604014	20.927463
72.819412	2395.806866	20.932480
72.849749	2389.246126	20.937498
72.788819	2381.257379	20.942515
72.807494	2382.563399	20.947533
72.767612	2370.872070	20.952551
73.001766	2398.650290	20.957568
73.081224	2399.775145	20.962586
73.138324	2405.363414	20.967603
72.969115	2410.692815	20.972621
73.102857	2401.876214	20.977639
73.294483	2411.980748	20.982656
73.105850	2402.619342	20.987674
73.369991	2403.346628	20.992691
73.329140	2404.154019	20.997709
73.289193	2402.364802	21.002727
73.429288	2409.659276	21.007744
73.208708	2409.485377	21.012762
73.677660	2409.956612	21.017779
73.873184	2437.441384	21.022797
74.000721	2426.998341	21.027815
73.736710	2430.125527	21.032832
73.996196	2437.906739	21.037850
73.984207	2426.847254	21.042867
73.917713	2435.867390	21.047885
73.872065	2425.558156	21.052903
74.115893	2447.260243	21.057920
74.074387	2450.284301	21.062938
74.607931	2458.291609	21.067955
74.115189	2472.175481	21.072973
74.735352	2451.890124	21.077991
74.858840	2458.612288	21.083008
75.022777	2465.328003	21.088026
75.274863	2451.235833	21.093043
75.101686	2453.993793	21.098061
75.112225	2446.792769	21.103079
74.941766	2461.364608	21.108096
75.174607	2448.243781	21.113114
75.746240	2448.795389	21.118131
75.128157	2457.721027	21.123149
75.091556	2452.085718	21.128167
75.426021	2450.440502	21.133184
75.427316	2457.245079	21.138202
75.714821	2467.926650	21.143219
75.394515	2476.680528	21.148237
75.553873	2478.078959	21.153255
76.111266	2480.600847	21.158272
75.770149	2476.765008	21.163290
75.807416	2479.314004	21.168307
75.875063	2479.955433	21.173325
76.048658	2470.812298	21.178343
76.294781	2475.563424	21.183360
76.031628	2471.254220	21.188378
76.129225	2466.959846	21.193395
76.364781	2471.788953	21.198413
76.367152	2495.346605	21.203431
76.738295	2500.637840	21.208448
76.830820	2504.029101	21.213466
76.882901	2501.292316	21.218483
76.396554	2490.768582	21.223501
76.558352	2494.598713	21.228519
76.788111	2513.115157	21.233536
76.594800	2504.706186	21.238554
76.585840	2500.085851	21.243571
76.830205	2511.177847	21.248589
77.021379	2507.268904	21.253607
77.297572	2516.709527	21.258624
77.321205	2528.887606	21.263642
77.654086	2521.071947	21.268659
77.465763	2525.938786	21.273677
77.691798	2526.813740	21.278695
77.792518	2521.466414	21.283712
77.377372	2530.517044	21.288730
77.598301	2509.713214	21.293747
77.620836	2524.779768	21.298765
77.693329	2526.659284	21.303783
77.902590	2525.986572	21.308800
77.632281	2547.220990	21.313818
78.205062	2546.050603	21.318835
78.119782	2547.989894	21.323853
78.601635	2539.970339	21.328871
78.401000	2537.752091	21.333888
78.161482	2555.228853	21.338906
78.586946	2537.053356	21.343923
78.590540	2533.020941	21.348941
78.391563	2538.094779	21.353959
78.621845	2534.988192	21.358976
79.008748	2549.502690	21.363994
79.336534	2559.216708	21.369011
79.248790	2563.661644	21.374029
79.207431	2556.655261	21.379047
79.501959	2542.001697	21.384064
79.382464	2559.011760	21.389082
79.413696	2538.841448	21.394099
79.741927	2544.206402	21.399117
79.268514	2544.708379	21.404135
79.689289	2545.897583	21.409152
79.742302	2560.134194	21.414170
79.622194	2552.335704	21.419187
79.629099	2554.317713	21.424205
79.564613	2548.035528	21.429223
79.819826	2556.180885	21.434240
79.612850	2553.763068	21.439258
79.873739	2550.857680	21.444275
79.937582	2559.716308	21.449293
80.149720	2573.073330	21.454311
80.218554	2585.400777	21.459328
80.164484	2582.945196	21.464346
80.576685	2570.166920	21.469363
80.148957	2586.010909	21.474381
80.331744	2580.108520	21.479399
80.487115	2572.849725	21.484416
80.189471	2581.567802	21.489434
80.426016	2600.842324	21.494451
80.804981	2607.782597	21.499469
80.744555	2614.957345	21.504487
80.777424	2613.141543	21.509504
80.983466	2611.225757	21.514522
81.373201	2612.880067	21.519539
81.325901	2634.484920	21.524557
81.259035	2635.482893	21.529575
81.415512	2632.677519	21.534592
81.326920	2637.180820	21.539610
81.535611	2625.123999	21.544627
82.094878	2627.295587	21.549645
81.717072	2632.451466	21.554663
82.272936	2622.622724	21.559680
82.078560	2635.424024	21.564698
82.088629	2620.355599	21.569715
82.290628	2629.471472	21.574733
81.901401	2632.321343	21.579751
82.330284	2617.561325	21.584768
82.142583	2619.024560	21.589786
82.216698	2636.832892	21.594803
82.320183	2634.655796	21.599821
82.545514	2656.218773	21.604839
82.414499	2649.007975	21.609856
82.502832	2645.275074	21.614874
82.648469	2646.639527	21.619891
82.729426	2649.180011	21.624909
82.790977	2667.641675	21.629927
83.348353	2675.137957	21.634944
83.041513	2687.973758	21.639962
83.239401	2673.904963	21.644979
83.272179	2683.261022	21.649997
83.246053	2687.489297	21.655015
83.470758	2672.009027	21.660032
83.136709	2679.496457	21.665050
83.657303	2672.863693	21.670067
83.596040	2673.951233	21.675085
83.751665	2688.375329	21.680103
84.265497	2698.119549	21.685120
83.974393	2693.238169	21.690138
83.884418	2692.480241	21.695155
84.392546	2698.611013	21.700173
84.357764	2692.667766	21.705191
84.750437	2691.110778	21.710208
84.345969	2688.853435	21.715226
84.521370	2690.473505	21.720243
84.318997	2685.972055	21.725261
84.082257	2696.772801	21.730279
84.451057	2686.037815	21.735296
84.382213	2707.189206	21.740314
84.287631	2707.283098	21.745331
84.633817	2714.877584	21.750349
84.621584	2723.796427	21.755367
84.723019	2721.048583	21.760384
85.100173	2741.782796	21.765402
85.490644	2733.760407	21.770419
85.490225	2749.291794	21.775437
85.337246	2744.713228	21.780455
85.707489	2744.052589	21.785472
85.773521	2733.666332	21.790490
85.759648	2746.294210	21.795507
86.199568	2735.665833	21.800525
85.716783	2735.624991	21.805543
86.399539	2729.666402	21.810560
85.981993	2744.764041	21.815578
85.924071	2743.239581	21.820595
85.999824	2738.958838	21.825613
85.779104	2738.965084	21.830631
86.272136	2736.113095	21.835648
86.363281	2734.251014	21.840666
86.461023	2759.164117	21.845683
86.670889	2747.791340	21.850701
86.395561	2763.122743	21.855719
87.095889	2758.736092	21.860736
86.985430	2766.947752	21.865754
87.212521	2760.118702	21.870771
87.145908	2764.406944	21.875789
87.043373	2760.613210	21.880807
87.070331	2762.853983	21.885824
87.031333	2760.846685	21.890842
86.943761	2768.699944	21.895859
87.270473	2777.622185	21.900877
87.486028	2788.272206	21.905895
87.670686	2797.936058	21.910912
87.499753	2794.817105	21.915930
87.659890	2796.283877	21.920947
87.937390	2791.522586	21.925965
87.695804	2793.722814	21.930983
88.231542	2794.814261	21.936000
88.302102	2816.789950	21.941018
88.352545	2822.669693	21.946035
88.508230	2818.624742	21.951053
88.138835	2818.363660	21.956071
88.396265	2815.822965	21.961088
88.155620	2822.723719	21.966106
88.340563	2820.926114	21.971123
88.295065	2814.057134	21.976141
88.144133	2849.271140	21.981159
88.731733	2841.651453	21.986176
88.732674	2846.541701	21.991194
88.901053	2849.005351	21.996211
88.973085	2850.365830	22.001229
88.664452	2876.929717	22.006247
89.223115	2878.837933	22.011264
89.487702	2883.841105	22.016282
89.479572	2891.444996	22.021299
89.774913	2880.494258	22.026317
89.461959	2879.283405	22.031335
89.997640	2885.375254	22.036352
89.953610	2877.507821	22.041370
89.676790	2879.155985	22.046387
89.589165	2884.636158	22.051405
89.881146	2891.034317	22.056423
90.455681	2895.866141	22.061440
90.524591	2908.086871	22.066458
90.725306	2906.912084	22.071475
90.466478	2899.682215	22.076493
90.611423	2910.688903	22.081511
90.636727	2906.857437	22.086528
90.894327	2894.260069	22.091546
90.669590	2892.986377	22.096563
90.519404	2906.229225	22.101581
90.713515	2892.996975	22.106599
91.048867	2915.807637	22.111616
90.860589	2925.479135	22.116634
90.885606	2938.017596	22.121651
91.051215	2920.167030	22.126669
91.155406	2932.864338	22.131687
91.314737	2929.429961	22.136704
91.731404	2941.804494	22.141722
91.773441	2956.746461	22.146739
91.895655	2953.166972	22.151757
91.459776	2961.695723	22.156775
92.153374	2950.388017	22.161792
91.850002	2949.358908	22.166810
91.982655	2952.026495	22.171827
92.199303	2940.195474	22.176845
92.089131	2965.126355	22.181863
92.233604	2974.400286	22.186880
92.632410	2983.198672	22.191898
92.491756	2975.868899	22.196915
92.802344	2974.922004	22.201933
92.590822	2976.907442	22.206951
93.068245	2962.198333	22.211968
92.982255	2979.906761	22.216986
92.801778	2977.755237	22.222003
93.130461	2997.197295	22.227021
93.282355	3006.260041	22.232039
93.288607	3004.329658	22.237056
93.727349	3000.427513	22.242074
93.438297	3009.564517	22.247091
94.085625	2993.608260	22.252109
93.759667	2993.698937	22.257127
93.672171	2992.850925	22.262144
94.001019	2999.788368	22.267162
94.019648	3001.167604	22.272179
94.321003	2992.153224	22.277197
94.258267	2994.239219	22.282215
94.097121	2993.439136	22.287232
94.029931	3005.950671	22.292250
94.019479	3019.522161	22.297267
94.248707	3020.505189	22.302285
94.362692	3039.204380	22.307303
94.522115	3029.507816	22.312320
94.604875	3024.424323	22.317338
94.517457	3041.843584	22.322355
94.807706	3045.979817	22.327373
94.649476	3059.147785	22.332391
94.795705	3063.312497	22.337408
95.198303	3060.249115	22.342426
95.338207	3048.258766	22.347443
95.343179	3039.688072	22.352461
95.649304	3063.899850	22.357479
95.703452	3070.299048	22.362496
95.862088	3086.312001	22.367514
95.834736	3076.460340	22.372531
96.122303	3076.085827	22.377549
95.938076	3083.286841	22.382567
96.071687	3079.606391	22.387584
96.311158	3068.752524	22.392602
96.333156	3076.059088	22.397619
96.233862	3073.472981	22.402637
96.443759	3076.784302	22.407655
96.245350	3062.569886	22.412672
96.791963	3077.882232	22.417690
96.862664	3087.393757	22.422707
96.713963	3088.571572	22.427725
96.871733	3094.866942	22.432743
96.901123	3087.297610	22.437760
97.030766	3095.759847	22.442778
96.947522	3084.788314	22.447795
97.161927	3087.399626	22.452813
96.995096	3098.885665	22.457831
97.254411	3108.223174	22.462848
97.647412	3111.131663	22.467866
97.184822	3124.555894	22.472883
97.596551	3110.119842	22.477901
97.916401	3129.480106	22.482919
97.837221	3139.317625	22.487936
98.037288	3144.043279	22.492954
98.186448	3153.580092	22.497971
98.424515	3133.827487	22.502989
98.165391	3141.732690	22.508007
98.517127	3129.942900	22.513024
98.696556	3130.392692	22.518042
98.471497	3138.166603	22.523059
98.686458	3148.518858	22.528077
98.868456	3168.366830	22.533095
98.942894	3161.186728	22.538112
99.291249	3158.201198	22.543130
98.800162	3162.085285	22.548147
99.419547	3165.214904	22.553165
99.060453	3168.911180	22.558183
98.861910	3174.507477	22.563200
99.400130	3176.811515	22.568218
99.464436	3192.337771	22.573235
99.557008	3187.102414	22.578253
99.705776	3184.978585	22.583271
99.755000	3192.712716	22.588288
100.164764	3188.620063	22.593306
100.504606	3186.280121	22.598323
100.642580	3184.577278	22.603341
100.276107	3174.933022	22.608359
100.239207	3190.577676	22.613376
100.455835	3171.441996	22.618394
100.380684	3196.011351	22.623411
100.603859	3200.053705	22.628429
100.889396	3206.447526	22.633447
100.520088	3208.451865	22.638464
100.938284	3211.201394	22.643482
100.814322	3211.661815	22.648499
100.882442	3209.152818	22.653517
101.179556	3217.619883	22.658535
101.046761	3241.270303	22.663552
101.423005	3238.939493	22.668570
101.287842	3240.435313	22.673587
101.717052	3238.758385	22.678605
101.630000	3229.875025	22.683623
101.586587	3244.355799	22.688640
102.175224	3257.319882	22.693658
102.362410	3261.960315	22.698675
102.675302	3261.234862	22.703693
102.622647	3266.427205	22.708711
102.623928	3268.351212	22.713728
102.659452	3262.522379	22.718746
102.925773	3264.939803	22.723763
102.977407	3260.444075	22.728781
103.018769	3253.124465	22.733799
102.828492	3265.799802	22.738816
103.092070	3266.244831	22.743834
102.822373	3264.414272	22.748851
102.738494	3259.302210	22.753869
103.415906	3251.767893	22.758887
102.979330	3251.488408	22.763904
103.133751	3270.224711	22.768922
103.301455	3283.545422	22.773939
103.549823	3277.618923	22.778957
103.591170	3286.256608	22.783975
103.321649	3286.608093	22.788992
103.594865	3301.873030	22.794010
103.780478	3306.447652	22.799027
104.221297	3306.806207	22.804045
104.341907	3309.353070	22.809063
103.996771	3321.300358	22.814080
104.659977	3315.687623	22.819098
104.381489	3332.074979	22.824115
104.724106	3341.481949	22.829133
104.837416	3334.250725	22.834151
104.985600	3336.698014	22.839168
105.109586	3337.807189	22.844186
104.848118	3341.888329	22.849203
105.188946	3331.943168	22.854221
105.408866	3329.897646	22.859239
105.360937	3343.864004	22.864256
105.705815	3347.398500	22.869274
106.094121	3352.555949	22.874291
105.866766	3351.530418	22.879309
106.016451	3354.156033	22.884327
106.163413	3353.553792	22.889344
106.354473	3356.010766	22.894362
106.042901	3360.000786	22.899379
106.116327	3358.037619	22.904397
106.317998	3355.449089	22.909415
105.895027	3362.734724	22.914432
106.133538	3349.683770	22.919450
106.045058	3366.250104	22.924467
106.469115	3384.663516	22.929485
106.516921	3385.968913	22.934503
106.282434	3385.941954	22.939520
106.794686	3395.765561	22.944538
106.962648	3416.057405	22.949555
106.890201	3413.233328	22.954573
107.367487	3402.486815	22.959591
107.273425	3414.025998	22.964608
107.939021	3429.333901	22.969626
107.970896	3432.713026	22.974643
108.153842	3442.564010	22.979661
108.224997	3435.462172	22.984679
108.195428	3444.900246	22.989696
107.960148	3442.393183	22.994714
108.099538	3443.459792	22.999731
107.924135	3438.491270	23.004749
108.401265	3429.211817	23.009767
108.086660	3436.565162	23.014784
108.425684	3447.753694	23.019802
108.828898	3459.757168	23.024819
108.911812	3465.486466	23.029837
108.970836	3469.409549	23.034855
108.939637	3458.026682	23.039872
108.885825	3471.098132	23.044890
108.876724	3477.719985	23.049907
109.188840	3476.968688	23.054925
109.422341	3462.936722	23.059943
109.267528	3484.386132	23.064960
109.584465	3480.008499	23.069978
109.832076	3496.086376	23.074995
109.888492	3506.414613	23.080013
110.192915	3492.805527	23.085031
110.391793	3503.039459	23.090048
110.506291	3495.241594	23.095066
110.853870	3495.929677	23.100083
110.601165	3495.297558	23.105101
111.008619	3488.627414	23.110119
111.082539	3496.953244	23.115136
111.221897	3485.813756	23.120154
111.249541	3488.248829	23.125171
110.963573	3485.301464	23.130189
110.802799	3485.131382	23.135207
111.169769	3489.540267	23.140224
111.290016	3476.709438	23.145242
111.549981	3483.880715	23.150259
111.312041	3500.104466	23.155277
111.655474	3498.496255	23.160295
111.479918	3513.368084	23.165312
111.776540	3515.260757	23.170330
112.003218	3514.025147	23.175347
111.782428	3522.651286	23.180365
111.965921	3524.326012	23.185383
111.868765	3535.643954	23.190400
111.795197	3541.871003	23.195418
112.418931	3545.861376	23.200435
112.142224	3552.168808	23.205453
112.870683	3556.857531	23.210471
112.954649	3568.351925	23.215488
112.747906	3567.951610	23.220506
112.933204	3559.539073	23.225523
113.145329	3564.418696	23.230541
113.174178	3558.899169	23.235559
113.453081	3574.161125	23.240576
113.832833	3576.377228	23.245594
113.869260	3576.539120	23.250611
113.935218	3590.800631	23.255629
114.403684	3575.068145	23.260647
113.995890	3586.289351	23.265664
114.121495	3581.281430	23.270682
114.469946	3579.437208	23.275699
114.278625	3574.055835	23.280717
114.704160	3574.333454	23.285735
114.567039	3570.193399	23.290752
114.448843	3581.512372	23.295770
114.770568	3566.223359	23.300787
114.615953	3584.911020	23.305805
115.041663	3589.828960	23.310823
114.990330	3613.852440	23.315840
114.883954	3607.262611	23.320858
115.353805	3599.243616	23.325875
115.309999	3605.732614	23.330893
115.488328	3600.527486	23.335911
115.549831	3631.349184	23.340928
115.548540	3633.492334	23.345946
115.832329	3635.228956	23.350963
115.563431	3637.050570	23.355981
116.060371	3634.576165	23.360999
116.011177	3651.680907	23.366016
116.274385	3660.082841	23.371034
116.180925	3667.021874	23.376051
116.493998	3666.072970	23.381069
116.656073	3664.658071	23.386087
116.434520	3680.557673	23.391104
116.713178	3686.393504	23.396122
116.894258	3691.735157	23.401139
116.550294	3696.953656	23.406157
117.047797	3696.083895	23.411175
116.953319	3721.728615	23.416192
117.245312	3723.299532	23.421210
117.521051	3724.978451	23.426227
117.499705	3721.955011	23.431245
117.754272	3725.065059	23.436263
117.760127	3731.093087	23.441280
117.944347	3741.486853	23.446298
118.133537	3750.481183	23.451315
117.919614	3751.138467	23.456333
118.259859	3739.675694	23.461351
118.618637	3749.173176	23.466368
118.587539	3747.439806	23.471386
119.058711	3764.411351	23.476403
118.724562	3782.946966	23.481421
119.296470	3767.433773	23.486439
119.500247	3777.623065	23.491456
119.294355	3764.883326	23.496474
119.453297	3765.766700	23.501491
119.515918	3764.248869	23.506509
119.586979	3765.880982	23.511527
119.850445	3766.547094	23.516544
119.976285	3763.643343	23.521562
120.212357	3756.777790	23.526579
120.040144	3759.210953	23.531597
120.129336	3751.762324	23.536615
119.987019	3781.230778	23.541632
120.212849	3791.109771	23.546650
120.701054	3781.056636	23.551667
120.337541	3799.941505	23.556685
120.616648	3797.754325	23.561703
120.947343	3808.126353	23.566720
120.851632	3827.052721	23.571738
121.029996	3827.936935	23.576755
120.866576	3832.984307	23.581773
120.900487	3825.925979	23.586791
120.994250	3833.619521	23.591808
121.153109	3854.248536	23.596826
121.915230	3843.565625	23.601843
121.723127	3855.288345	23.606861
122.053938	3849.552999	23.611879
122.224735	3863.130194	23.616896
122.200880	3873.714564	23.621914
122.306489	3884.304256	23.626931
122.618713	3872.402966	23.631949
122.541059	3868.873221	23.636967
122.742576	3883.720692	23.641984
122.633976	3879.263700	23.647002
123.134332	3871.655831	23.652019
122.759671	3876.772303	23.657037
122.636789	3897.631957	23.662055
123.385613	3903.430659	23.667072
123.137744	3908.920248	23.672090
123.231456	3901.981358	23.677107
123.376953	3919.565901	23.682125
123.659622	3926.703097	23.687143
123.807536	3932.043834	23.692160
123.593684	3937.484743	23.697178
124.298721	3916.457762	23.702195
124.036640	3923.861971	23.707213
123.961761	3924.707911	23.712231
124.205804	3935.200045	23.717248
124.507880	3957.072090	23.722266
125.057830	3950.347550	23.727283
124.755759	3960.715968	23.732301
124.846616	3947.069722	23.737319
124.291387	3956.041294	23.742336
124.769838	3977.952895	23.747354
125.169697	3981.631393	23.752371
125.277184	3980.796280	23.757389
125.522645	3981.788590	23.762407
125.687557	4001.837083	23.767424
125.775512	4017.109500	23.772442
126.118594	4003.830468	23.777459
126.107868	3996.975053	23.782477
126.150048	4003.137426	23.787495
126.374934	4003.429748	23.792512
126.386023	4007.657975	23.797530
126.969693	4013.608137	23.802547
126.765607	4027.538688	23.807565
126.895843	4025.339816	23.812583
126.989131	4030.082002	23.817600
127.130930	4027.528864	23.822618
127.251132	4031.952882	23.827635
127.184291	4036.555407	23.832653
127.239254	4024.577020	23.837671
127.533423	4044.955023	23.842688
127.523121	4059.524934	23.847706
128.174347	4058.758081	23.852723
127.740995	4060.822301	23.857741
127.558124	4070.806778	23.862759
127.784791	4076.985388	23.867776
127.972702	4084.262065	23.872794
128.162474	4092.396695	23.877811
127.998977	4091.415991	23.882829
128.484170	4117.846877	23.887847
128.550890	4113.803173	23.892864
128.646411	4129.876108	23.897882
128.731599	4130.954560	23.902899
128.895083	4149.495452	23.907917
129.210808	4138.444559	23.912935
129.413142	4149.617668	23.917952
129.357667	4151.711321	23.922970
129.780666	4155.906945	23.927987
129.928520	4171.158170	23.933005
129.939532	4175.504458	23.938023
130.492634	4164.037306	23.943040
130.320246	4186.332273	23.948058
130.345669	4170.068794	23.953075
130.675854	4167.766430	23.958093
130.730201	4178.791668	23.963111
130.685012	4175.108779	23.968128
130.604349	4177.356705	23.973146
131.197334	4183.933998	23.978163
131.096657	4200.566150	23.983181
131.163543	4206.081962	23.988199
131.220656	4193.299909	23.993216
131.074630	4191.589533	23.998234
131.342169	4197.155158	24.003251
131.255100	4210.334835	24.008269
131.340863	4222.804137	24.013287
131.798381	4224.978049	24.018304
131.907698	4223.831111	24.023322
132.171110	4246.686795	24.028339
132.189010	4250.405818	24.033357
132.581519	4252.993662	24.038375
132.695609	4245.842107	24.043392
132.176924	4254.565735	24.048410
132.544575	4267.844446	24.053427
133.489753	4280.299471	24.058445
133.043285	4282.591585	24.063463
133.207864	4273.735118	24.068480
133.372306	4282.249921	24.073498
133.865462	4275.804907	24.078515
133.713826	4294.851716	24.083533
134.010247	4288.543483	24.088551
134.212828	4276.059122	24.093568
134.252567	4290.828177	24.098586
134.633661	4287.425778	24.103603
134.587133	4279.638229	24.108621
134.739359	4287.047352	24.113639
134.592178	4289.534037	24.118656
134.410744	4286.292141	24.123674
134.717321	4295.251569	24.128691
134.786978	4312.511196	24.133709
134.753537	4316.773360	24.138727
135.234611	4320.059032	24.143744
135.106985	4339.508779	24.148762
135.368368	4348.282711	24.153779
135.197347	4350.105321	24.158797
135.239902	4360.610225	24.163815
135.716107	4371.274908	24.168832
135.707078	4382.690370	24.173850
135.968069	4373.668999	24.178867
136.073921	4403.526290	24.183885
136.108060	4408.388952	24.188903
136.687767	4399.566119	24.193920
136.556389	4417.342519	24.198938
136.798295	4426.204565	24.203955
136.997298	4435.086832	24.208973
136.829360	4435.913026	24.213991
137.526622	4431.677432	24.219008
137.457309	4433.888186	24.224026
137.806819	4445.248097	24.229043
137.902041	4453.202122	24.234061
138.210203	4459.773826	24.239079
138.182769	4451.255463	24.244096
138.094746	4462.195055	24.249114
138.404378	4462.860921	24.254131
138.511668	4456.210677	24.259149
138.405693	4455.112213	24.264167
138.713856	4444.517785	24.269184
138.762991	4452.410718	24.274202
138.740986	4445.475078	24.279219
138.835819	4466.282728	24.284237
138.903087	4482.260646	24.289255
139.421208	4473.578966	24.294272
139.299653	4475.241088	24.299290
139.444566	4477.800014	24.304307
139.794745	4484.475952	24.309325
139.867589	4496.909786	24.314343
140.348906	4494.950653	24.319360
140.266193	4505.199511	24.324378
140.377044	4505.417988	24.329395
140.597555	4496.435252	24.334413
140.354865	4494.027520	24.339431
140.853871	4495.924241	24.344448
140.948664	4519.246994	24.349466
140.831659	4528.728027	24.354483
141.230624	4515.443559	24.359501
141.071172	4523.022864	24.364519
141.166883	4522.883455	24.369536
141.008068	4528.270962	24.374554
141.466984	4544.319445	24.379571
141.732510	4546.836337	24.384589
141.539406	4563.712563	24.389607
141.889760	4573.811383	24.394624
141.860146	4586.986955	24.399642
142.047194	4584.566537	24.404659
142.409698	4595.876504	24.409677
142.506194	4606.810381	24.414695
142.873333	4604.968564	24.419712
143.101937	4611.932994	24.424730
143.205002	4609.236463	24.429747
143.530535	4606.673594	24.434765
143.483928	4622.297720	24.439783
143.868699	4631.757808	24.444800
143.664522	4640.883069	24.449818
143.783311	4631.530208	24.454835
144.033833	4633.489385	24.459853
144.188491	4642.136549	24.464871
144.274763	4642.813654	24.469888
144.159636	4644.540064	24.474906
144.311481	4653.770620	24.479923
144.508652	4661.768290	24.484941
144.551200	4673.514030	24.489959
144.403059	4667.628965	24.494976
145.017366	4686.140342	24.499994
144.942088	4701.061888	24.505011
145.125967	4689.960019	24.510029
145.239253	4697.531324	24.515047
145.440609	4704.094210	24.520064
145.520690	4710.474257	24.525082
145.381792	4712.653667	24.530099
145.498064	4718.153930	24.535117
145.921908	4733.411293	24.540135
146.510353	4733.485961	24.545152
146.738688	4745.771700	24.550170
146.141763	4745.430418	24.555187
146.686286	4745.838569	24.560205
146.913738	4770.499189	24.565223
147.080795	4759.138768	24.570240
147.338133	4766.721753	24.575258
147.319976	4768.669510	24.580275
147.995362	4754.745221	24.585293
147.992793	4758.824010	24.590311
147.875042	4751.032621	24.595328
147.909966	4765.748640	24.600346
147.760957	4780.792160	24.605363
147.787153	4789.111388	24.610381
148.025227	4787.872287	24.615399
148.320261	4803.335137	24.620416
148.363872	4822.056481	24.625434
148.445359	4816.498194	24.630451
148.503069	4824.893447	24.635469
148.924306	4847.795704	24.640487
149.566291	4841.572168	24.645504
149.794846	4835.139213	24.650522
149.519673	4837.777777	24.655539
149.800014	4838.719745	24.660557
149.703583	4851.351585	24.665575
150.080409	4861.841307	24.670592
150.194876	4868.855528	24.675610
150.549783	4865.959091	24.680627
150.475007	4861.721402	24.685645
150.393546	4862.706116	24.690663
150.840292	4883.755615	24.695680
151.152751	4893.674250	24.700698
150.983492	4907.511180	24.705715
151.303702	4905.686252	24.710733
150.970133	4903.600544	24.715751
151.390776	4915.152447	24.720768
151.634740	4930.749447	24.725786
151.583865	4933.216162	24.730803
151.982974	4932.025321	24.735821
151.905133	4942.240664	24.740839
151.490987	4954.326144	24.745856
152.106866	4944.756933	24.750874
152.460887	4962.831062	24.755891
152.383938	4972.921198	24.760909
152.662116	4984.506887	24.765927
152.941322	4988.406281	24.770944
153.051629	4990.689962	24.775962
153.180128	5009.557710	24.780979
153.456281	5015.631276	24.785997
153.584644	5023.668438	24.791015
153.964804	5021.767066	24.796032
154.033915	5012.891551	24.801050
153.983077	5011.622977	24.806067
154.123734	5007.166017	24.811085
154.055428	5020.099547	24.816103
154.481500	5032.024364	24.821120
154.368673	5037.610054	24.826138
154.416196	5035.691705	24.831155
155.030792	5032.992201	24.836173
154.671979	5063.009889	24.841191
155.191862	5077.506495	24.846208
155.415323	5068.994970	24.851226
155.372402	5066.766913	24.856243
155.785243	5066.861721	24.861261
155.754743	5088.733416	24.866279
156.112486	5087.696276	24.871296
156.173407	5086.325697	24.876314
156.103112	5082.651303	24.881331
156.294508	5098.200221	24.886349
156.772076	5116.729228	24.891367
156.487322	5124.051897	24.896384
156.634174	5120.021889	24.901402
156.704234	5128.106167	24.906419
156.949122	5133.736340	24.911437
156.960741	5145.750152	24.916455
157.251834	5150.047346	24.921472
157.766222	5172.885696	24.926490
157.740064	5179.594427	24.931507
158.098124	5164.594562	24.936525
158.179710	5172.385154	24.941543
158.150569	5186.066260	24.946560
158.514110	5187.290005	24.951578
158.757288	5200.421054	24.956595
158.864490	5196.380040	24.961613
158.782013	5206.255655	24.966631
159.284058	5207.334589	24.971648
159.199879	5218.561281	24.976666
159.219733	5229.136510	24.981683
159.455460	5224.126209	24.986701
159.985501	5230.618826	24.991719
159.716124	5250.196223	24.996736
160.161783	5255.773189	25.001754
159.934151	5255.022912	25.006771
160.466328	5255.829559	25.011789
160.510350	5276.388412	25.016807
160.729995	5277.353463	25.021824
161.111965	5276.418655	25.026842
160.945042	5281.792781	25.031859
161.160375	5284.385465	25.036877
161.258054	5305.813786	25.041895
161.070762	5318.747668	25.046912
161.438946	5308.043140	25.051930
161.624310	5314.348444	25.056947
161.883937	5329.546075	25.061965
162.133786	5343.616326	25.066983
162.105888	5341.922380	25.072000
162.365455	5338.817626	25.077018
162.434091	5353.970210	25.082035
162.598485	5349.125440	25.087053
162.789753	5361.205189	25.092071
162.807520	5360.226962	25.097088
162.943532	5359.141767	25.102106
162.688063	5380.938052	25.107123
163.238570	5385.876046	25.112141
163.757898	5401.266786	25.117159
163.855336	5414.477910	25.122176
164.098466	5417.885960	25.127194
164.053249	5425.263416	25.132211
164.700137	5415.404165	25.137229
164.596019	5422.496774	25.142247
164.507087	5429.882777	25.147264
164.885166	5437.314687	25.152282
164.771445	5445.467780	25.157299
165.135383	5455.929301	25.162317
165.109909	5459.146530	25.167335
165.562332	5460.636204	25.172352
165.875786	5464.195905	25.177370
166.103621	5477.293459	25.182387
166.176908	5465.779087	25.187405
166.387842	5467.691981	25.192423
166.288961	5471.754854	25.197440
166.338331	5475.629663	25.202458
166.609409	5490.662780	25.207475
166.983980	5496.059211	25.212493
166.992647	5500.284319	25.217511
166.929207	5504.610614	25.222528
167.207719	5528.004013	25.227546
167.416180	5528.760806	25.232563
167.284492	5532.245955	25.237581
167.779293	5545.576360	25.242599
167.679435	5567.061734	25.247616
168.192065	5558.286681	25.252634
168.259222	5578.138134	25.257651
168.373371	5577.073718	25.262669
168.399210	5588.395652	25.267687
168.639770	5583.445826	25.272704
169.138895	5590.233056	25.277722
169.087870	5614.993780	25.282739
169.330308	5613.333011	25.287757
169.863461	5605.360282	25.292775
169.388913	5616.894984	25.297792
169.715755	5621.033204	25.302810
170.034358	5641.335575	25.307827
170.026016	5639.444938	25.312845
170.351618	5647.918317	25.317863
170.237477	5661.606335	25.322880
170.734798	5672.363014	25.327898
170.471502	5683.919943	25.332915
170.584044	5685.293112	25.337933
170.861928	5675.310003	25.342951
170.792616	5702.021769	25.347968
171.379851	5706.554351	25.352986
171.485731	5704.532201	25.358003
171.391904	5724.233288	25.363021
171.577893	5728.387703	25.368039
171.728837	5745.166360	25.373056
172.104760	5753.443743	25.378074
172.266937	5770.374053	25.383091
172.439751	5768.736171	25.388109
172.552890	5771.660724	25.393127
172.835195	5791.778697	25.398144
173.313881	5797.670813	25.403162
173.348716	5796.590705	25.408179
173.541443	5795.445298	25.413197
173.797497	5814.866493	25.418215
173.760515	5826.934240	25.423232
174.014798	5820.831128	25.428250
173.982681	5823.073135	25.433267
173.957650	5836.655843	25.438285
174.474861	5841.828250	25.443303
174.343628	5845.838951	25.448320
174.802848	5860.382983	25.453338
175.283337	5872.140098	25.458355
175.322458	5878.056703	25.463373
175.448673	5877.118584	25.468391
175.348082	5873.949199	25.473408
175.632729	5895.434321	25.478426
175.389972	5897.934938	25.483443
175.570469	5916.550874	25.488461
176.138833	5926.405804	25.493479
176.330579	5942.698257	25.498496
176.566196	5940.354060	25.503514
176.958348	5959.631798	25.508531
177.404206	5955.187259	25.513549
177.510077	5965.451118	25.518567
177.003072	5962.341795	25.523584
177.628720	5963.909331	25.528602
177.956635	5982.399567	25.533619
177.855825	5995.504351	25.538637
178.194427	5984.310756	25.543655
178.143552	5994.120490	25.548672
178.117863	5995.207319	25.553690
178.536147	6011.696609	25.558707
178.493630	6026.013968	25.563725
178.572314	6011.238751	25.568743
178.518725	6044.785596	25.573760
179.011734	6040.047919	25.578778
179.304658	6058.818410	25.583795
179.173061	6073.185422	25.588813
179.819850	6075.855793	25.593831
180.122842	6083.053747	25.598848
180.239217	6099.483487	25.603866
180.428030	6112.869491	25.608883
180.115167	6109.961277	25.613901
180.496708	6102.405056	25.618919
180.575481	6124.293118	25.623936
180.749786	6131.451033	25.628954
181.124772	6138.735095	25.633971
181.025304	6144.896560	25.638989
181.359709	6141.300566	25.644007
181.466654	6154.849148	25.649024
181.650285	6160.144879	25.654042
181.859565	6173.187790	25.659059
182.228711	6199.138183	25.664077
182.544776	6184.084193	25.669095
182.240509	6209.846938	25.674112
182.838215	6208.406404	25.679130
182.786499	6224.395740	25.684148
182.597181	6215.821918	25.689165
183.169342	6233.463935	25.694183
183.499468	6253.530854	25.699200
183.962393	6236.753960	25.704218
184.103693	6252.222391	25.709236
183.954292	6265.346962	25.714253
184.539100	6276.101939	25.719271
184.321297	6276.338230	25.724288
184.417126	6280.973736	25.729306
184.941154	6291.827321	25.734324
184.984394	6306.228051	25.739341
185.386745	6303.961069	25.744359
185.415342	6296.391002	25.749376
185.698926	6309.709360	25.754394
185.944430	6314.490170	25.759412
186.081363	6324.312664	25.764429
186.127782	6324.084326	25.769447
186.271729	6333.092177	25.774464
186.310199	6346.134938	25.779482
186.805377	6354.101752	25.784500
186.456659	6357.657103	25.789517
186.745264	6367.051036	25.794535
186.676643	6381.666370	25.799552
187.185065	6378.154298	25.804570
187.118210	6402.358672	25.809588
187.192627	6422.267536	25.814605
187.649184	6423.744068	25.819623
187.847346	6440.155639	25.824640
188.154870	6441.742482	25.829658
188.630276	6450.238073	25.834676
189.147450	6466.596449	25.839693
189.485521	6466.064329	25.844711
189.581776	6466.380368	25.849728
189.457015	6459.335852	25.854746
189.641952	6470.029629	25.859764
189.758481	6473.975031	25.864781
189.995083	6484.893470	25.869799
190.021307	6484.600687	25.874816
190.233771	6483.028003	25.879834
190.589154	6482.029705	25.884852
190.555354	6500.307607	25.889869
190.810910	6507.045195	25.894887
190.981955	6521.616946	25.899904
191.051626	6516.827814	25.904922
191.078999	6525.833126	25.909940
191.104532	6529.040094	25.914957
191.476795	6533.136714	25.919975
191.649079	6549.513192	25.924992
191.594859	6563.157082	25.930010
191.981838	6568.264754	25.935028
192.118197	6590.008207	25.940045
192.236517	6590.015455	25.945063
192.310579	6609.240116	25.950080
192.410090	6623.027924	25.955098
193.088847	6632.562028	25.960116
193.227560	6649.512035	25.965133
193.378571	6667.457761	25.970151
193.659868	6668.321811	25.975168
193.717415	6669.636964	25.980186
193.952093	6687.164173	25.985204
194.228660	6698.876572	25.990221
194.347735	6698.971035	25.995239
194.480595	6713.752058	26.000256
194.689131	6714.460910	26.005274
195.167779	6722.987616	26.010292
194.969789	6750.832748	26.015309
195.790747	6752.244136	26.020327
195.524626	6769.232862	26.025344
195.881397	6772.287146	26.030362
196.048899	6778.745420	26.035380
196.085942	6792.727457	26.040397
196.368847	6798.525307	26.045415
196.732006	6811.530872	26.050432
196.736063	6814.158303	26.055450
197.226333	6832.075315	26.060468
196.978281	6842.537049	26.065485
197.275850	6843.292297	26.070503
197.693797	6845.667270	26.075520
197.731175	6867.730620	26.080538
198.296861	6873.205670	26.085556
198.109961	6886.693979	26.090573
198.263254	6880.335876	26.095591
198.596914	6902.470847	26.100608
198.771353	6907.010615	26.105626
199.050552	6903.711216	26.110644
199.253408	6915.492190	26.115661
199.716034	6929.919504	26.120679
199.872127	6936.496113	26.125696
199.669902	6932.718763	26.130714
200.185314	6938.320663	26.135732
200.088262	6945.706352	26.140749
200.386456	6933.258804	26.145767
200.822840	6961.691649	26.150784
200.966348	6971.389994	26.155802
201.099538	6980.776052	26.160820
201.187075	6979.593826	26.165837
201.216622	6980.401255	26.170855
201.454302	6984.813730	26.175872
201.699117	7000.497762	26.180890
201.970260	6994.693622	26.185908
202.136331	7014.371507	26.190925
202.069018	7028.220909	26.195943
202.313755	7046.478679	26.200960
202.702626	7041.407949	26.205978
202.650698	7052.800052	26.210996
202.730370	7075.803509	26.216013
202.733052	7078.061401	26.221031
203.447019	7096.895120	26.226048
203.143083	7113.498431	26.231066
203.334437	7129.221022	26.236084
203.664207	7145.002604	26.241101
204.023049	7158.448997	26.246119
204.376283	7168.123475	26.251136
204.690046	7184.853414	26.256154
204.989804	7193.361705	26.261172
205.089976	7191.440979	26.266189
205.378373	7198.761406	26.271207
206.011464	7211.344250	26.276224
205.915008	7220.274520	26.281242
206.101775	7224.552768	26.286260
206.126019	7223.582828	26.291277
206.538088	7238.587380	26.296295
206.647871	7249.096209	26.301312
206.575246	7259.949645	26.306330
207.223841	7273.585208	26.311348
206.944672	7291.907925	26.316365
207.115310	7285.048035	26.321383
208.033752	7299.587156	26.326400
208.192329	7313.457461	26.331418
208.302491	7307.445177	26.336436
208.747793	7301.552567	26.341453
208.701630	7326.290192	26.346471
209.101866	7323.657523	26.351488
208.828432	7333.285671	26.356506
209.456272	7330.539603	26.361524
209.408144	7332.490114	26.366541
209.538773	7359.265043	26.371559
209.992074	7351.072797	26.376576
210.009039	7358.678923	26.381594
210.163066	7365.951614	26.386612
210.327247	7377.469238	26.391629
210.268702	7395.203762	26.396647
210.779187	7396.066726	26.401664
210.832901	7419.150389	26.406682
211.440449	7415.266628	26.411700
211.337551	7420.457423	26.416717
211.362890	7430.097799	26.421735
211.922361	7437.719761	26.426752
211.885395	7442.386246	26.431770
212.469167	7453.677305	26.436788
212.127875	7472.867803	26.441805
212.377595	7465.202087	26.446823
212.799401	7470.391862	26.451840
213.001897	7493.794196	26.456858
213.043057	7489.279184	26.461876
213.597997	7500.096476	26.466893
213.119277	7517.711260	26.471911
213.833596	7514.017392	26.476928
213.710790	7532.191153	26.481946
214.296838	7542.500723	26.486964
214.324742	7545.802741	26.491981
214.954742	7556.999956	26.496999
215.067200	7583.098351	26.502016
214.954526	7589.599288	26.507034
215.264765	7572.448671	26.512052
215.613414	7592.799292	26.517069
215.480685	7613.737352	26.522087
216.049261	7617.405623	26.527104
216.102429	7630.277996	26.532122
216.079995	7646.052530	26.537140
216.600104	7660.587061	26.542157
216.905526	7672.825183	26.547175
217.258708	7672.818595	26.552192
217.189397	7681.095661	26.557210
217.498206	7693.111367	26.562228
217.805282	7696.711190	26.567245
217.893420	7705.677630	26.572263
218.410719	7726.933968	26.577280
218.162170	7740.543035	26.582298
218.207714	7733.068679	26.587316
218.558508	7755.089672	26.592333
218.581868	7765.278231	26.597351
218.788358	7782.643630	26.602368
218.633813	7812.092152	26.607386
219.319207	7815.461728	26.612404
219.832394	7841.731959	26.617421
220.164247	7861.785047	26.622439
220.225713	7864.542785	26.627456
220.596760	7866.927767	26.632474
220.825348	7876.581666	26.637492
221.367911	7884.118429	26.642509
221.274438	7883.603922	26.647527
221.772060	7894.206386	26.652544
221.800019	7898.655719	26.657562
222.049857	7904.334954	26.662580
222.518100	7911.605817	26.667597
222.334981	7930.357006	26.672615
222.423333	7920.598547	26.677632
222.757615	7948.024278	26.682650
223.203241	7957.664873	26.687668
223.386894	7965.472139	26.692685
223.399215	7964.168060	26.697703
223.738182	7974.683355	26.702720
223.805209	7988.649933	26.707738
224.297184	7985.737352	26.712756
224.681541	7994.968340	26.717773
224.278755	7996.855089	26.722791
224.989532	8007.210412	26.727808
224.837279	8024.587648	26.732826
224.854983	8021.262813	26.737844
225.164193	8033.925538	26.742861
225.476557	8044.266504	26.747879
225.938765	8044.747708	26.752896
225.922555	8071.948633	26.757914
226.211717	8086.769841	26.762932
226.269407	8079.302031	26.767949
226.497716	8115.161350	26.772967
226.678174	8105.731163	26.777984
227.071367	8128.578462	26.783002
227.519177	8142.294054	26.788020
227.783905	8138.928238	26.793037
227.907461	8153.137758	26.798055
228.099995	8163.450699	26.803072
227.942353	8170.583049	26.808090
228.804456	8178.685146	26.813108
229.244490	8188.241014	26.818125
229.346091	8203.816169	26.823143
229.542458	8202.189222	26.828160
229.681777	8208.469271	26.833178
229.786013	8221.278931	26.838196
230.042536	8232.806103	26.843213
229.983158	8237.067232	26.848231
230.132142	8239.747350	26.853248
230.574624	8246.828127	26.858266
230.824105	8273.935128	26.863284
231.179102	8278.598402	26.868301
231.352784	8284.352089	26.873319
231.569114	8301.564656	26.878336
231.865978	8326.823678	26.883354
231.888394	8317.586947	26.888372
232.112519	8335.260999	26.893389
232.304262	8348.009605	26.898407
232.573991	8346.896587	26.903424
232.703454	8375.479039	26.908442
232.600587	8383.050891	26.913460
233.387143	8390.320425	26.918477
233.245682	8403.603381	26.923495
233.493319	8428.604455	26.928512
233.891450	8444.002750	26.933530
233.963183	8455.755884	26.938548
234.359656	8468.759957	26.943565
234.538978	8475.790338	26.948583
235.190270	8491.691672	26.953600
235.282867	8504.964551	26.958618
235.323283	8515.085198	26.963636
235.911377	8526.126158	26.968653
236.118013	8540.859073	26.973671
236.567049	8541.723255	26.978688
236.800632	8552.441862	26.983706
237.134687	8544.686216	26.988724
237.167950	8547.238870	26.993741
237.161001	8562.861606	26.998759
237.346038	8546.515159	27.003776
237.676218	8561.811096	27.008794
237.830474	8577.378246	27.013812
238.227048	8580.430503	27.018829
238.141984	8592.926787	27.023847
238.465171	8591.824115	27.028864
238.544228	8609.664048	27.033882
238.830131	8633.150091	27.038900
239.126742	8639.184914	27.043917
239.216495	8653.089867	27.048935
239.502486	8667.853929	27.053952
239.586007	8681.385730	27.058970
239.611973	8703.585423	27.063988
240.218090	8697.165379	27.069005
240.481266	8714.596009	27.074023
240.794028	8729.299208	27.079040
241.387296	8733.764900	27.084058
241.174708	8754.179830	27.089076
241.780199	8757.308198	27.094093
241.516543	8770.424462	27.099111
241.853517	8782.806408	27.104128
241.697342	8797.508495	27.109146
241.731921	8817.704299	27.114164
242.591332	8826.343466	27.119181
243.105805	8845.900556	27.124199
243.082108	8839.040641	27.129216
243.416594	8862.561007	27.134234
243.689743	8891.889961	27.139252
244.149280	8885.471959	27.144269
243.847521	8908.453277	27.149287
244.595325	8918.093936	27.154304
245.051513	8932.709943	27.159322
245.101877	8944.942560	27.164340
245.175352	8939.340735	27.169357
245.471676	8945.832928	27.174375
246.031253	8967.017414	27.179392
245.845145	8976.751910	27.184410
246.042836	9007.517050	27.189428
246.692764	8993.667663	27.194445
246.892959	9019.415815	27.199463
247.352561	9022.734326	27.204480
247.383885	9034.365302	27.209498
247.174483	9040.120546	27.214516
247.504209	9062.278642	27.219533
247.665465	9066.031104	27.224551
248.070189	9080.098712	27.229568
248.252754	9098.199724	27.234586
248.701006	9115.041028	27.239604
249.079460	9107.555409	27.244621
249.146091	9122.143601	27.249639
249.756811	9146.860969	27.254656
250.073650	9152.965961	27.259674
249.913270	9151.935619	27.264692
250.356730	9144.139012	27.269709
250.445252	9170.967974	27.274727
250.724106	9181.857663	27.279744
250.708138	9185.375967	27.284762
250.882750	9202.032782	27.289780
251.184568	9207.585405	27.294797
251.490913	9229.596386	27.299815
251.648661	9241.125134	27.304832
251.974328	9249.816982	27.309850
251.923727	9262.854462	27.314868
252.315942	9278.713740	27.319885
252.850976	9281.905394	27.324903
252.868863	9293.034681	27.329920
253.401938	9300.426135	27.334938
253.022030	9321.513010	27.339956
253.608080	9322.273953	27.344973
253.612722	9354.698756	27.349991
254.075339	9364.531542	27.355008
254.445705	9381.596463	27.360026
254.606701	9404.165598	27.365044
254.706358	9415.355126	27.370061
255.133483	9421.287620	27.375079
255.407145	9442.516001	27.380096
255.782774	9452.839994	27.385114
256.238843	9476.288432	27.390132
256.640521	9483.966519	27.395149
256.754139	9491.186491	27.400167
257.185724	9507.554793	27.405184
257.476162	9510.734732	27.410202
257.367810	9513.088600	27.415220
258.097195	9520.073102	27.420237
258.334394	9535.192059	27.425255
258.292876	9555.329769	27.430272
258.691059	9554.813159	27.435290
258.857137	9574.599874	27.440308
259.416819	9566.259628	27.445325
259.525136	9576.607040	27.450343
259.749987	9598.167647	27.455360
260.100099	9599.306970	27.460378
260.275470	9611.152697	27.465396
260.280695	9624.286649	27.470413
260.472930	9631.445759	27.475431
260.314333	9646.103811	27.480448
260.964098	9665.747043	27.485466
260.825589	9686.787289	27.490484
261.166562	9688.277878	27.495501
261.476538	9722.007579	27.500519
261.446806	9735.331742	27.505536
262.316040	9746.471238	27.510554
262.400910	9761.665072	27.515572
262.998484	9775.714399	27.520589
263.130484	9778.410882	27.525607
263.221655	9795.105267	27.530624
263.590885	9815.159748	27.535642
263.875344	9821.283556	27.540660
264.192613	9826.791846	27.545677
264.573061	9845.809722	27.550695
264.729135	9848.855335	27.555712
265.029857	9858.570635	27.560730
264.909308	9869.576042	27.565748
265.509841	9861.976741	27.570765
265.850114	9879.275642	27.575783
266.174571	9897.219643	27.580800
266.090098	9902.657431	27.585818
266.060223	9928.471365	27.590836
266.406128	9929.874233	27.595853
266.540869	9955.427455	27.600871
266.744411	9976.153092	27.605888
267.358906	9991.597587	27.610906
267.285234	10000.308676	27.615924
267.831572	10031.879716	27.620941
267.935424	10037.958035	27.625959
268.004547	10057.378372	27.630976
268.665205	10077.760168	27.635994
268.883160	10095.065438	27.641012
269.271219	10108.708951	27.646029
269.637767	10130.399229	27.651047
269.763589	10146.150795	27.656064
270.385389	10150.549417	27.661082
270.665427	10163.395282	27.666100
271.047991	10185.374270	27.671117
271.276550	10187.846885	27.676135
271.934677	10201.042136	27.681152
272.518425	10201.738575	27.686170
272.384129	10211.468755	27.691188
272.849744	10211.952260	27.696205
272.929411	10211.720140	27.701223
273.064390	10213.601700	27.706240
273.272632	10227.224012	27.711258
273.345360	10237.505544	27.716276
273.551501	10234.671165	27.721293
273.941698	10261.055378	27.726311
273.644529	10265.934208	27.731328
274.298128	10274.960792	27.736346
274.120274	10300.360600	27.741364
274.615089	10305.708946	27.746381
274.930464	10326.401894	27.751399
275.045012	10348.195223	27.756416
275.918477	10344.471000	27.761434
276.154614	10369.844675	27.766452
276.047662	10382.326653	27.771469
276.605687	10408.525400	27.776487
276.827983	10413.136134	27.781504
277.482975	10422.531687	27.786522
277.211136	10439.346826	27.791540
277.467553	10454.863048	27.796557
277.888615	10467.642621	27.801575
277.915532	10473.690096	27.806592
278.358514	10488.855912	27.811610
278.309892	10500.109235	27.816628
278.709222	10523.725366	27.821645
279.163210	10543.088916	27.826663
279.455069	10547.873943	27.831680
279.662483	10552.946308	27.836698
279.578979	10571.632969	27.841716
280.230111	10596.719334	27.846733
280.653143	10596.706353	27.851751
280.580405	10618.721564	27.856768
281.404276	10631.276126	27.861786
281.420777	10642.057202	27.866804
281.710060	10647.070903	27.871821
282.178999	10659.754471	27.876839
282.097848	10672.418703	27.881856
282.683301	10687.787882	27.886874
282.826200	10698.554359	27.891892
283.009263	10711.069474	27.896909
283.498930	10719.360635	27.901927
283.224822	10742.049144	27.906944
283.712030	10744.247275	27.911962
284.105632	10770.429578	27.916980
284.403237	10788.621326	27.921997
284.593109	10801.872667	27.927015
284.928599	10820.359054	27.932032
285.416218	10826.854239	27.937050
285.529950	10851.128314	27.942068
285.857243	10867.307351	27.947085
286.508223	10864.438151	27.952103
286.495424	10891.383137	27.957120
286.822387	10901.927600	27.962138
287.207684	10917.386373	27.967156
287.265628	10926.755427	27.972173
287.492293	10944.417595	27.977191
287.826354	10965.081292	27.982208
288.187196	10962.355520	27.987226
288.435906	10992.038373	27.992244
288.762371	11018.077552	27.997261
288.950090	11016.186069	28.002279
289.429474	11038.864706	28.007296
289.566755	11063.063356	28.012314
289.869786	11070.599795	28.017332
290.021272	11085.552567	28.022349
290.543325	11096.374585	28.027367
290.462270	11122.390362	28.032384
291.176124	11133.551345	28.037402
290.944420	11164.397219	28.042420
291.362004	11171.464873	28.047437
291.830443	11192.326258	28.052455
292.257594	11216.822883	28.057472
292.623680	11228.266431	28.062490
292.760057	11244.020611	28.067508
293.177830	11256.950133	28.072525
293.501690	11277.134217	28.077543
293.532382	11289.743754	28.082560
294.028350	11294.686950	28.087578
294.445420	11305.005226	28.092596
294.802783	11333.359435	28.097613
295.131825	11338.332008	28.102631
295.120284	11344.954994	28.107648
295.488239	11363.401457	28.112666
295.832492	11369.884315	28.117684
296.009398	11372.115476	28.122701
296.445255	11398.172899	28.127719
296.491290	11401.041575	28.132736
296.959826	11415.645847	28.137754
297.221306	11426.007503	28.142772
297.345161	11443.555601	28.147789
297.710422	11451.362108	28.152807
298.189659	11482.907543	28.157824
298.251959	11499.190496	28.162842
298.758547	11505.257553	28.167860
299.090113	11513.788436	28.172877
299.564130	11528.696927	28.177895
299.473549	11554.407227	28.182912
299.849153	11558.828204	28.187930
300.435370	11580.529637	28.192948
300.564121	11593.119468	28.197965
300.867370	11591.770670	28.202983
301.078065	11616.477962	28.208000
301.372703	11634.316243	28.213018
301.936374	11644.764863	28.218036
302.154967	11671.013816	28.223053
302.271696	11667.445128	28.228071
302.559302	11687.347870	28.233088
303.144010	11703.988529	28.238106
303.229654	11705.778185	28.243124
303.569553	11727.481903	28.248141
304.037836	11735.144043	28.253159
304.217549	11751.554946	28.258176
304.194577	11766.902186	28.263194
304.648086	11778.536069	28.268212
304.889805	11795.536881	28.273229
305.021250	11821.240578	28.278247
305.507084	11842.833246	28.283264
305.654775	11863.565661	28.288282
305.943170	11876.147597	28.293300
306.239201	11895.575454	28.298317
306.752119	11910.516690	28.303335
307.240956	11939.847516	28.308352
307.279927	11950.968715	28.313370
307.783977	11969.529802	28.318388
308.230856	11981.405941	28.323405
308.694923	11996.709627	28.328423
308.730270	12012.094257	28.333440
309.428112	12016.975610	28.338458
309.485138	12030.209654	28.343476
309.773770	12044.899490	28.348493
310.325736	12052.265697	28.353511
310.550655	12076.320754	28.358528
310.604807	12085.313923	28.363546
310.984659	12091.943720	28.368564
311.262186	12098.908205	28.373581
311.804328	12113.801696	28.378599
311.837938	12135.503857	28.383616
312.018150	12138.897917	28.388634
312.531579	12140.821918	28.393652
312.599744	12171.559273	28.398669
312.887997	12172.101430	28.403687
313.361357	12194.222757	28.408704
313.618978	12193.293419	28.413722
313.769664	12216.871357	28.418740
313.814143	12227.018252	28.423757
313.995445	12245.954813	28.428775
314.504485	12272.957610	28.433792
314.773848	12288.620451	28.438810
315.378802	12312.734358	28.443828
315.318650	12332.844501	28.448845
315.849378	12349.097783	28.453863
316.144006	12370.687051	28.458880
316.518958	12398.271856	28.463898
316.840813	12420.357646	28.468916
317.240163	12433.080371	28.473933
317.831704	12446.838405	28.478951
317.820179	12469.397912	28.483968
318.254205	12483.610843	28.488986
318.594306	12491.565550	28.494004
318.874062	12530.786752	28.499021
319.214968	12553.486002	28.504039
319.425199	12561.757004	28.509056
319.566358	12593.641608	28.514074
320.267523	12602.172053	28.519092
320.336413	12624.450962	28.524109
320.666211	12645.569441	28.529127
320.810714	12673.617107	28.534144
321.096037	12683.538391	28.539162
321.608438	12698.125110	28.544180
321.566221	12724.211432	28.549197
322.172871	12739.666312	28.554215
323.018597	12768.630558	28.559232
323.253221	12770.648080	28.564250
323.444714	12788.900871	28.569268
323.490910	12808.729630	28.574285
324.250738	12831.556159	28.579303
324.679827	12841.004989	28.584320
324.765402	12860.111850	28.589338
325.411797	12869.397959	28.594356
325.300581	12906.704016	28.599373
325.870855	12915.902518	28.604391
326.227043	12928.984189	28.609408
325.933107	12948.430291	28.614426
326.913089	12956.979864	28.619444
327.093881	12990.226616	28.624461
327.348013	12989.714377	28.629479
327.766067	13015.898251	28.634496
327.727279	13040.469737	28.639514
328.656864	13041.897758	28.644532
328.566746	13048.461004	28.649549
329.048126	13073.255633	28.654567
329.642428	13085.370279	28.659584
329.725656	13096.985683	28.664602
330.282916	13097.690445	28.669620
330.184840	13127.361128	28.674637
330.465769	13121.866771	28.679655
330.536232	13156.509351	28.684672
330.747042	13179.894028	28.689690
331.036958	13185.346130	28.694708
331.640464	13210.544409	28.699725
331.535171	13220.449392	28.704743
332.117704	13255.323864	28.709760
332.307018	13286.723270	28.714778
332.675229	13304.948024	28.719796
333.013775	13332.508648	28.724813
333.484427	13353.937642	28.729831
334.148416	13359.966005	28.734848
334.120219	13401.646814	28.739866
335.076443	13416.815349	28.744884
335.180854	13433.181727	28.749901
335.380028	13443.509044	28.754919
335.936765	13475.743402	28.759936
336.367115	13480.885131	28.764954
336.392813	13492.483833	28.769972
336.585867	13518.227419	28.774989
337.448180	13535.715047	28.780007
337.856324	13559.773657	28.785024
337.820530	13576.121995	28.790042
338.162475	13582.589550	28.795060
338.678508	13599.147017	28.800077
339.072621	13623.594558	28.805095
339.405569	13638.786892	28.810112
339.359190	13660.120135	28.815130
339.653812	13681.804770	28.820148
339.964259	13704.074212	28.825165
340.637442	13717.101614	28.830183
341.284762	13730.020093	28.835200
341.338307	13759.605358	28.840218
341.747479	13762.475349	28.845236
341.856826	13788.566492	28.850253
342.030701	13800.398625	28.855271
342.742889	13830.485963	28.860288
342.988200	13853.209478	28.865306
343.406967	13862.428083	28.870324
343.644100	13891.404197	28.875341
343.825945	13907.130675	28.880359
344.914277	13923.658194	28.885376
344.301846	13955.239793	28.890394
344.871574	13965.394758	28.895412
345.172200	13989.055651	28.900429
345.633238	14005.469122	28.905447
346.032496	14029.523397	28.910464
346.267642	14041.867658	28.915482
346.898346	14046.846486	28.920500
346.581245	14082.900593	28.925517
346.921610	14095.482389	28.930535
347.747336	14125.526436	28.935552
347.820922	14141.944636	28.940570
348.086099	14153.006497	28.945588
348.536075	14177.600904	28.950605
348.751335	14199.204337	28.955623
349.410604	14218.645863	28.960640
349.802004	14241.113270	28.965658
350.258903	14249.085417	28.970676
350.497945	14269.049864	28.975693
350.742678	14286.532486	28.980711
351.734423	14294.740593	28.985728
351.819006	14310.468622	28.990746
352.078570	14341.100441	28.995764
352.507889	14338.061578	29.000781
352.678449	14356.166180	29.005799
353.092529	14373.763608	29.010816
353.181780	14394.701160	29.015834
353.992837	14402.817583	29.020852
354.064429	14424.720737	29.025869
354.337921	14437.942449	29.030887
354.933369	14471.835420	29.035904
354.633356	14488.110335	29.040922
355.316081	14508.906105	29.045940
355.447551	14532.202868	29.050957
355.502472	14564.627257	29.055975
356.400657	14590.597987	29.060992
356.530448	14622.582127	29.066010
357.154213	14629.553608	29.071028
357.143841	14660.192678	29.076045
357.682523	14681.855755	29.081063
358.801539	14698.746274	29.086080
358.685591	14725.989916	29.091098
359.586616	14729.268208	29.096116
359.903315	14743.370002	29.101133
359.847456	14774.146341	29.106151
360.348457	14784.135391	29.111168
360.610448	14792.695060	29.116186
361.121766	14803.025018	29.121204
361.391119	14824.996417	29.126221
361.298823	14858.164214	29.131239
362.184268	14867.879205	29.136256
362.379622	14877.918701	29.141274
362.796529	14907.247435	29.146292
363.285681	14918.011322	29.151309
363.635214	14948.706775	29.156327
364.182327	14947.810755	29.161344
364.198375	14977.725835	29.166362
364.663363	14983.347986	29.171380
365.210840	15016.300607	29.176397
365.032202	15029.201960	29.181415
365.617506	15041.692660	29.186432
365.723376	15065.717389	29.191450
365.777161	15085.131939	29.196468
366.258205	15106.970322	29.201485
366.297353	15132.595320	29.206503
366.845303	15152.557646	29.211520
366.981889	15176.721621	29.216538
367.726693	15205.511369	29.221556
368.126396	15240.052371	29.226573
368.376347	15257.052494	29.231591
368.639287	15285.080474	29.236608
369.244998	15302.299389	29.241626
369.732486	15311.936975	29.246644
369.939752	15351.851160	29.251661
369.995125	15378.690579	29.256679
370.626606	15385.126344	29.261696
371.039950	15432.181235	29.266714
371.645305	15456.098338	29.271732
371.933945	15464.852132	29.276749
371.991847	15497.688768	29.281767
372.922694	15514.886122	29.286784
373.191582	15526.547098	29.291802
373.792489	15554.763203	29.296820
374.136295	15563.470769	29.301837
374.572549	15596.714068	29.306855
375.249247	15610.834869	29.311872
375.474909	15626.577192	29.316890
375.578274	15639.670194	29.321908
376.035929	15656.464462	29.326925
376.105217	15678.194508	29.331943
376.719604	15693.379071	29.336960
376.995857	15718.460949	29.341978
377.129937	15736.612457	29.346996
377.698538	15758.525402	29.352013
377.897215	15777.079390	29.357031
378.593098	15801.467763	29.362048
378.512872	15826.160340	29.367066
378.987203	15838.588193	29.372084
379.534033	15870.160497	29.377101
379.692548	15907.801680	29.382119
380.267683	15910.005287	29.387136
380.836667	15939.958709	29.392154
380.948767	15959.478733	29.397172
381.606054	15980.950173	29.402189
381.804269	16005.126295	29.407207
382.291136	16024.376867	29.412224
382.519333	16049.811085	29.417242
382.699134	16066.264017	29.422260
383.480168	16088.211877	29.427277
383.490992	16116.222406	29.432295
384.195960	16136.722628	29.437312
384.510071	16178.180864	29.442330
385.033484	16189.985912	29.447348
385.678113	16202.411919	29.452365
385.584751	16229.803125	29.457383
386.374619	16251.907271	29.462400
386.740806	16278.353596	29.467418
387.159881	16288.552139	29.472436
387.530406	16302.287883	29.477453
387.698192	16324.671560	29.482471
387.979248	16333.914892	29.487488
388.367337	16350.526446	29.492506
388.634142	16367.851746	29.497524
388.761534	16397.383581	29.502541
389.131423	16418.233407	29.507559
390.089055	16434.351191	29.512576
389.952671	16469.179870	29.517594
390.201537	16491.576851	29.522612
390.714876	16511.310372	29.527629
391.211355	16539.392291	29.532647
391.341764	16561.901546	29.537664
391.647719	16596.089221	29.542682
391.902361	16617.109042	29.547700
392.679148	16644.349721	29.552717
393.227265	16670.377023	29.557735
393.509674	16702.162250	29.562752
394.194863	16726.913212	29.567770
394.337150	16751.088985	29.572788
394.843584	16759.194998	29.577805
395.243627	16797.041768	29.582823
395.832288	16819.400626	29.587840
396.538963	16848.475497	29.592858
396.423068	16871.910393	29.597876
396.960161	16893.779199	29.602893
397.089916	16911.145845	29.607911
397.757226	16933.529144	29.612928
398.103427	16966.966806	29.617946
398.379567	16987.379822	29.622964
398.734773	17004.717931	29.627981
399.181428	17030.934043	29.632999
399.636493	17060.384814	29.638016
400.368735	17085.156215	29.643034
400.624056	17112.549124	29.648052
401.108734	17127.854299	29.653069
401.050467	17159.804197	29.658087
401.723226	17178.878770	29.663104
401.826212	17217.153800	29.668122
402.265201	17243.944486	29.673140
402.736994	17268.954719	29.678157
403.322498	17296.149285	29.683175
403.586195	17318.232721	29.688192
404.076207	17340.217530	29.693210
403.996984	17375.657603	29.698228
404.880283	17400.132228	29.703245
405.154850	17432.782361	29.708263
405.791336	17444.183965	29.713280
406.172808	17484.421462	29.718298
406.322451	17509.760177	29.723316
407.320998	17521.831664	29.728333
407.325457	17543.520534	29.733351
407.675449	17573.712613	29.738368
408.174700	17595.240430	29.743386
408.914712	17614.459152	29.748404
409.518433	17630.070252	29.753421
409.686106	17666.187755	29.758439
409.551120	17668.154605	29.763456
409.923098	17688.390292	29.768474
409.909591	17717.639829	29.773492
410.814373	17740.346486	29.778509
410.929366	17777.644645	29.783527
411.340054	17803.130425	29.788544
411.776285	17826.778772	29.793562
412.220517	17859.196082	29.798580
412.412090	17889.828575	29.803597
412.739384	17928.627869	29.808615
413.304436	17962.307605	29.813632
413.938032	17989.209711	29.818650
414.036205	18013.905497	29.823668
414.592350	18041.428685	29.828685
415.273220	18074.127628	29.833703
415.555337	18105.205560	29.838720
416.225453	18123.485675	29.843738
416.487580	18162.735303	29.848756
416.767992	18192.713694	29.853773
416.830554	18230.818139	29.858791
417.654892	18263.662730	29.863808
418.264783	18289.650243	29.868826
418.550273	18326.686726	29.873844
419.090756	18334.960591	29.878861
419.541260	18380.034295	29.883879
420.241129	18397.505267	29.888896
420.934085	18430.372329	29.893914
421.248103	18456.143880	29.898932
421.982141	18469.784658	29.903949
421.763860	18499.626174	29.908967
422.266993	18517.815646	29.913984
423.166680	18537.316379	29.919002
423.106505	18564.772560	29.924020
423.677075	18584.019097	29.929037
424.304736	18617.535554	29.934055
424.153380	18636.908215	29.939072
424.587270	18661.714532	29.944090
425.102367	18686.371724	29.949108
425.435885	18712.108309	29.954125
425.989497	18752.147644	29.959143
426.650081	18778.810596	29.964160
427.149166	18792.103654	29.969178
427.455690	18820.651101	29.974196
428.078891	18832.688945	29.979213
428.098412	18869.658468	29.984231
428.622396	18901.763663	29.989248
428.793629	18923.927901	29.994266
429.239661	18952.482102	29.999284
429.875716	18979.469006	30.004301
429.823974	19011.350403	30.009319
430.394808	19047.448215	30.014336
430.920675	19073.028757	30.019354
431.312661	19096.227801	30.024372
431.872361	19123.395633	30.029389
432.484125	19154.024297	30.034407
432.743379	19178.019063	30.039424
433.227290	19195.903717	30.044442
433.483402	19229.577159	30.049460
433.817484	19245.889983	30.054477
434.160347	19274.708867	30.059495
434.322243	19302.430191	30.064512
435.290728	19335.802153	30.069530
435.138219	19376.568640	30.074548
435.972621	19395.575314	30.079565
436.586193	19424.723807	30.084583
437.019048	19460.995755	30.089600
437.531626	19471.112214	30.094618
437.731646	19512.359536	30.099636
437.950411	19533.808353	30.104653
438.457121	19568.799788	30.109671
439.336709	19604.177594	30.114688
440.216198	19622.509987	30.119706
440.006929	19649.715824	30.124724
440.546661	19680.160921	30.129741
441.176448	19709.356187	30.134759
441.278682	19735.309283	30.139776
442.002806	19745.710748	30.144794
442.559477	19799.665364	30.149812
443.067331	19814.514348	30.154829
443.446854	19838.218893	30.159847
443.733287	19867.772737	30.164864
444.557395	19888.942501	30.169882
444.650577	19931.073785	30.174900
444.858930	19952.340959	30.179917
445.622158	19984.643756	30.184935
445.703569	20023.716605	30.189952
446.431324	20047.091938	30.194970
446.688519	20071.791239	30.199988
447.210896	20110.138852	30.205005
447.461203	20146.508022	30.210023
447.592780	20172.259112	30.215040
448.592719	20199.920556	30.220058
448.934560	20235.266959	30.225076
449.416101	20267.899905	30.230093
449.992292	20293.559485	30.235111
450.344727	20323.922675	30.240128
450.946065	20345.902670	30.245146
451.240914	20386.085476	30.250164
451.911860	20414.458862	30.255181
452.369987	20435.877078	30.260199
452.714394	20471.039722	30.265216
453.482020	20500.439735	30.270234
453.387238	20527.461898	30.275252
454.013759	20553.100498	30.280269
454.651342	20590.253600	30.285287
454.828245	20626.009898	30.290304
455.502548	20657.929380	30.295322
455.612802	20677.898801	30.300340
456.334055	20698.919496	30.305357
456.711178	20715.258107	30.310375
456.972258	20743.939164	30.315392
457.527065	20761.489075	30.320410
458.000648	20798.854264	30.325428
458.107498	20830.130537	30.330445
458.465704	20864.076709	30.335463
458.983245	20891.389401	30.340480
459.865346	20920.720776	30.345498
459.833462	20963.067703	30.350516
460.310483	20990.321658	30.355533
460.698803	21021.674745	30.360551
461.227181	21070.687400	30.365568
461.729677	21091.311118	30.370586
462.331791	21131.866637	30.375604
462.669488	21173.551988	30.380621
463.159075	21200.221523	30.385639
463.404112	21238.480235	30.390656
464.146957	21269.877351	30.395674
464.698151	21308.929346	30.400692
465.113848	21339.388773	30.405709
465.911888	21369.535325	30.410727
466.077589	21412.455245	30.415744
466.977975	21437.514548	30.420762
467.477390	21467.758483	30.425780
467.482775	21505.267680	30.430797
468.000918	21535.412680	30.435815
468.356508	21578.286259	30.440832
469.131194	21606.968181	30.445850
469.243169	21640.329933	30.450868
469.636693	21694.574992	30.455885
470.130818	21724.244549	30.460903
470.429086	21760.549171	30.465920
471.476357	21799.135860	30.470938
471.807454	21831.191171	30.475956
472.467152	21869.397952	30.480973
472.967780	21892.920526	30.485991
473.683496	21928.628197	30.491008
474.212493	21957.119929	30.496026
474.524029	21991.776921	30.501044
474.926362	22015.490183	30.506061
475.625641	22050.302901	30.511079
475.730543	22082.097052	30.516096
476.049212	22108.411803	30.521114
476.471047	22143.153154	30.526132
477.050090	22188.039744	30.531149
477.652629	22218.230888	30.536167
477.965140	22253.884610	30.541184
478.790933	22269.151533	30.546202
479.208510	22318.964663	30.551220
479.603227	22349.322274	30.556237
480.140736	22380.937050	30.561255
480.396958	22417.056131	30.566272
481.070461	22433.187853	30.571290
481.391075	22463.952869	30.576308
481.923319	22496.180688	30.581325
482.633163	22518.733610	30.586343
482.598392	22545.782746	30.591360
483.138353	22573.702828	30.596378
483.486305	22612.232805	30.601396
484.052867	22642.885737	30.606413
484.644906	22684.118698	30.611431
484.950219	22731.933922	30.616448
486.038363	22753.037545	30.621466
486.775077	22784.091323	30.626484
487.003698	22810.413715	30.631501
487.164979	22845.326504	30.636519
487.412341	22856.777948	30.641536
488.047694	22895.113177	30.646554
488.479186	22934.957000	30.651572
488.896062	22964.982246	30.656589
489.332196	23002.717005	30.661607
489.532406	23043.814058	30.666624
490.121625	23077.065003	30.671642
490.596198	23114.352826	30.676660
491.029201	23156.839502	30.681677
491.866575	23196.494085	30.686695
491.896577	23242.204439	30.691712
492.499773	23273.968068	30.696730
493.249053	23316.780494	30.701748
493.583345	23367.445890	30.706765
494.390658	23405.949512	30.711783
494.476197	23441.289199	30.716800
495.219936	23480.219800	30.721818
495.933363	23517.131038	30.726836
496.470453	23556.867445	30.731853
497.075640	23591.794649	30.736871
497.134526	23634.322515	30.741888
498.377875	23672.491876	30.746906
498.572940	23702.965808	30.751924
498.451177	23741.316581	30.756941
499.794835	23768.927996	30.761959
500.195488	23814.984236	30.766976
500.417676	23847.404410	30.771994
501.172505	23884.340627	30.777012
501.641606	23916.457733	30.782029
502.291904	23947.015570	30.787047
502.748691	23992.879066	30.792064
503.445598	24024.144057	30.797082
504.026848	24053.584346	30.802100
504.287081	24098.460979	30.807117
504.878662	24120.861742	30.812135
504.816392	24156.369924	30.817152
505.703092	24181.681543	30.822170
506.304253	24217.860838	30.827188
506.277336	24258.827862	30.832205
506.837324	24302.057501	30.837223
507.793546	24327.806479	30.842240
508.348743	24363.549953	30.847258
508.953644	24391.621225	30.852276
508.950239	24426.477077	30.857293
509.447402	24464.079555	30.862311
509.771184	24487.701121	30.867328
510.486752	24522.724645	30.872346
510.881017	24558.838424	30.877364
511.043526	24599.320847	30.882381
511.599387	24635.309804	30.887399
511.914898	24676.389556	30.892416
512.723146	24711.197862	30.897434
513.384467	24752.195150	30.902452
513.702927	24794.962825	30.907469
514.366625	24821.300374	30.912487
514.932729	24866.387240	30.917504
515.352420	24904.582867	30.922522
515.869087	24938.498360	30.927540
516.382163	24993.844783	30.932557
516.867695	25031.899462	30.937575
517.172810	25070.305946	30.942592
517.310942	25119.451596	30.947610
518.169629	25157.826033	30.952628
518.257856	25203.880128	30.957645
519.257620	25251.104681	30.962663
519.914414	25301.475137	30.967680
520.171094	25353.018645	30.972698
521.144016	25389.283961	30.977716
521.811549	25430.778288	30.982733
522.378969	25476.384222	30.987751
523.053977	25526.238867	30.992768
523.436962	25543.841958	30.997786
524.027306	25589.160968	31.002804
524.362016	25634.408179	31.007821
525.396582	25669.561443	31.012839
525.419692	25701.141886	31.017856
525.668246	25740.419232	31.022874
526.558639	25786.185722	31.027892
527.010795	25826.907132	31.032909
528.025744	25865.988648	31.037927
528.312253	25906.801246	31.042944
528.861155	25947.305092	31.047962
529.504033	25978.250873	31.052980
529.653749	26014.790550	31.057997
530.360112	26055.324730	31.063015
530.923502	26097.258054	31.068032
531.284667	26139.348173	31.073050
532.107225	26176.033126	31.078068
532.307495	26223.304406	31.083085
532.907700	26257.438639	31.088103
533.672739	26295.194189	31.093120
533.910701	26333.328428	31.098138
534.498682	26370.005501	31.103156
535.106735	26418.093946	31.108173
535.818558	26461.473831	31.113191
536.186254	26499.839897	31.118208
536.346685	26541.068095	31.123226
536.939719	26570.107007	31.128244
537.647786	26616.733693	31.133261
538.197349	26637.847949	31.138279
538.738127	26673.507501	31.143296
539.096565	26716.075407	31.148314
539.658846	26746.219331	31.153332
540.037722	26787.344822	31.158349
540.747651	26821.337513	31.163367
541.169092	26869.316014	31.168384
541.443517	26918.647931	31.173402
542.062771	26955.966593	31.178420
542.807312	27010.105299	31.183437
543.131520	27044.284382	31.188455
543.463304	27096.507725	31.193472
543.869721	27141.433411	31.198490
545.074420	27184.743041	31.203508
545.231643	27233.311476	31.208525
546.110744	27271.798031	31.213543
546.500287	27317.704613	31.218560
546.880591	27375.149287	31.223578
547.421789	27421.302238	31.228596
547.693852	27457.013422	31.233613
548.736336	27509.983656	31.238631
549.279093	27567.316472	31.243648
549.869467	27614.010492	31.248666
550.964222	27648.086235	31.253684
551.386757	27700.612222	31.258701
551.677025	27733.357165	31.263719
552.515315	27784.544005	31.268736
552.714328	27823.934385	31.273754
553.414545	27856.760821	31.278772
553.660036	27911.841620	31.283789
554.524263	27948.353017	31.288807
555.255682	27990.504814	31.293824
555.650722	28051.499735	31.298842
556.281634	28084.796223	31.303860
556.948093	28128.205161	31.308877
557.562935	28164.947442	31.313895
558.229427	28205.857400	31.318912
558.887527	28244.725004	31.323930
559.677070	28277.582191	31.328948
559.913103	28317.489462	31.333965
560.526661	28345.125854	31.338983
560.944045	28382.134874	31.344000
561.536641	28436.620095	31.349018
562.138780	28459.427086	31.354036
562.530691	28503.054101	31.359053
563.067303	28550.109220	31.364071
563.596188	28596.573199	31.369088
564.197951	28650.720453	31.374106
564.600027	28702.331093	31.379124
564.977172	28746.199064	31.384141
565.848547	28787.991844	31.389159
566.643856	28825.712266	31.394176
566.978042	28868.244793	31.399194
567.956007	28901.112632	31.404212
568.446815	28948.708841	31.409229
569.004299	28978.941225	31.414247
569.364707	29003.899137	31.419264
569.890899	29032.340125	31.424282
570.820282	29058.881060	31.429300
570.869139	29095.764458	31.434317
571.630904	29124.071957	31.439335
572.108331	29163.667082	31.444352
572.159429	29216.841798	31.449370
573.066262	29251.738807	31.454388
573.531695	29300.903367	31.459405
573.830849	29342.410509	31.464423
574.460594	29384.996594	31.469440
574.829010	29435.986143	31.474458
575.740292	29482.626559	31.479476
575.969081	29529.867501	31.484493
576.268024	29581.547789	31.489511
577.053666	29621.711120	31.494528
577.771280	29688.672944	31.499546
578.213426	29732.547408	31.504564
578.872177	29795.197847	31.509581
579.475628	29846.902968	31.514599
580.530819	29899.481868	31.519616
580.910012	29942.783825	31.524634
581.472780	29992.165058	31.529652
582.437807	30044.806067	31.534669
582.766030	30089.060531	31.539687
583.627896	30120.841436	31.544704
583.451921	30178.483921	31.549722
584.375510	30227.490048	31.554740
585.441869	30274.284545	31.559757
585.843411	30320.661839	31.564775
586.424481	30359.573570	31.569792
587.122674	30412.980074	31.574810
587.777716	30446.871720	31.579828
588.251169	30506.118727	31.584845
588.899138	30549.505565	31.589863
589.971177	30588.982656	31.594880
589.995452	30637.288512	31.599898
590.982661	30677.340391	31.604916
591.449477	30717.131680	31.609933
591.683929	30773.068669	31.614951
592.657400	30806.883554	31.619968
592.843984	30857.830856	31.624986
593.532318	30900.389505	31.630004
593.962504	30952.628483	31.635021
594.742601	30992.750373	31.640039
595.005152	31041.807495	31.645056
595.523863	31106.359199	31.650074
596.329988	31148.898158	31.655092
596.926258	31206.692343	31.660109
597.549547	31254.318311	31.665127
598.251032	31301.602563	31.670144
598.628105	31358.046819	31.675162
599.179758	31398.551251	31.680180
600.066235	31436.285271	31.685197
600.301122	31496.513209	31.690215
600.520402	31516.398764	31.695232
601.557410	31580.800438	31.700250
601.826350	31630.047433	31.705268
602.575264	31668.267275	31.710285
603.064655	31731.760654	31.715303
603.865309	31766.665782	31.720320
604.312858	31834.494263	31.725338
604.884430	31883.006622	31.730356
605.686263	31928.449957	31.735373
606.394360	31978.093013	31.740391
607.165730	32018.020211	31.745408
607.452787	32081.677987	31.750426
608.316820	32121.510296	31.755444
609.322452	32162.172853	31.760461
609.918297	32207.172189	31.765479
610.753890	32247.047160	31.770496
611.401856	32299.232094	31.775514
612.284421	32331.948681	31.780532
612.735178	32366.660201	31.785549
612.993435	32411.209483	31.790567
613.797738	32449.297804	31.795584
614.338038	32496.031130	31.800602
614.835656	32532.363745	31.805620
615.594147	32573.421327	31.810637
615.962301	32627.464499	31.815655
616.544093	32669.190402	31.820672
616.998047	32723.696239	31.825690
617.607014	32768.561042	31.830708
618.282087	32827.730723	31.835725
618.831800	32873.770080	31.840743
619.626792	32924.790813	31.845760
620.014554	32983.606446	31.850778
620.449123	33030.580375	31.855796
621.111536	33088.031744	31.860813
621.607572	33147.727604	31.865831
622.373302	33188.957379	31.870848
622.902897	33242.122516	31.875866
623.749516	33307.270593	31.880884
624.448958	33351.723775	31.885901
624.899963	33407.050423	31.890919
625.841752	33457.259706	31.895936
626.292681	33520.094598	31.900954
626.798941	33566.793816	31.905972
627.402202	33617.916582	31.910989
628.255137	33668.619854	31.916007
629.043931	33725.432246	31.921024
629.237310	33784.639504	31.926042
630.266300	33832.016006	31.931060
631.239013	33888.359873	31.936077
631.558109	33925.723376	31.941095
632.348896	33979.547599	31.946112
632.748752	34028.717843	31.951130
632.905760	34075.344855	31.956148
633.665277	34119.940287	31.961165
634.117251	34170.160381	31.966183
635.110554	34223.663096	31.971200
635.436641	34276.299625	31.976218
635.994305	34307.947932	31.981236
636.910398	34361.521714	31.986253
637.212935	34415.380970	31.991271
638.208050	34463.715231	31.996288
638.594382	34514.943094	32.001306
639.230686	34561.635438	32.006324
639.833351	34616.216826	32.011341
640.531386	34683.865767	32.016359
641.218707	34729.595158	32.021376
641.831424	34782.502923	32.026394
642.382137	34845.654834	32.031412
642.901413	34901.046527	32.036429
643.553937	34962.588904	32.041447
644.465189	35014.965902	32.046464
644.834889	35076.651479	32.051482
645.210648	35139.007884	32.056500
646.224082	35185.534722	32.061517
647.127551	35255.888412	32.066535
647.305119	35308.326420	32.071552
648.057705	35372.176502	32.076570
648.797945	35437.502797	32.081588
649.727980	35484.869827	32.086605
650.186529	35542.453591	32.091623
650.794173	35598.192966	32.096640
651.381707	35649.936164	32.101658
652.169487	35720.821021	32.106676
652.865630	35779.135520	32.111693
653.292222	35833.452550	32.116711
654.113306	35883.442458	32.121728
655.092098	35950.559954	32.126746
655.426217	36009.577705	32.131764
656.405983	36061.691685	32.136781
656.695302	36127.038882	32.141799
657.670919	36192.841446	32.146816
658.426288	36242.721500	32.151834
658.721290	36308.084262	32.156852
659.667255	36360.973917	32.161869
660.005160	36414.275883	32.166887
661.074450	36466.230248	32.171904
661.980302	36536.834896	32.176922
662.406742	36597.588440	32.181940
663.389354	36647.936445	32.186957
663.902613	36695.346475	32.191975
664.710145	36743.816549	32.196992
665.271383	36802.261727	32.202010
665.886916	36851.087466	32.207028
667.039033	36895.818578	32.212045
667.337165	36956.472453	32.217063
667.799069	36991.839847	32.222080
668.625028	37043.208833	32.227098
669.037289	37098.394656	32.232116
669.735811	37142.169118	32.237133
670.205326	37195.569276	32.242151
670.808522	37238.499901	32.247168
671.709029	37296.380364	32.252186
671.853195	37355.161909	32.257204
672.747546	37398.987843	32.262221
673.377386	37458.206399	32.267239
673.948966	37515.818356	32.272256
674.555700	37566.960549	32.277274
674.971334	37636.768099	32.282292
675.799663	37684.619519	32.287309
676.365199	37756.331979	32.292327
677.266748	37817.621299	32.297344
677.888920	37878.643142	32.302362
678.356524	37936.217908	32.307380
679.480431	37993.082904	32.312397
680.051398	38072.602153	32.317415
680.806455	38117.007144	32.322432
681.765845	38174.439767	32.327450
681.912240	38237.255726	32.332468
683.142768	38291.470027	32.337485
683.397496	38362.540787	32.342503
684.590584	38423.018008	32.347520
685.381771	38464.441251	32.352538
685.641040	38536.027616	32.357556
686.618327	38595.953263	32.362573
687.133886	38653.574870	32.367591
688.134881	38721.929783	32.372608
688.944706	38764.702097	32.377626
689.243357	38827.120724	32.382644
690.366228	38879.547055	32.387661
690.928633	38933.943917	32.392679
691.412209	38994.488858	32.397696
692.084769	39043.311865	32.402714
692.554304	39106.666166	32.407732
693.616721	39175.615475	32.412749
694.006742	39243.696074	32.417767
694.971076	39291.330135	32.422784
695.955195	39354.564003	32.427802
696.040175	39424.259699	32.432820
696.885905	39474.283160	32.437837
697.397202	39533.504208	32.442855
698.098736	39591.432104	32.447872
698.953154	39660.334507	32.452890
699.653013	39728.203717	32.457908
700.436288	39782.992309	32.462925
701.284202	39849.458659	32.467943
702.136408	39910.660921	32.472960
702.890291	39969.365486	32.477978
703.204239	40025.904255	32.482996
704.040562	40081.636236	32.488013
704.723334	40150.807646	32.493031
705.065282	40210.497974	32.498048
706.033621	40278.058550	32.503066
706.423374	40331.829799	32.508084
707.039463	40391.212184	32.513101
707.850405	40449.723240	32.518119
708.491925	40509.996115	32.523136
709.175780	40566.480931	32.528154
709.563649	40634.206307	32.533172
710.327065	40692.085518	32.538189
711.216147	40754.168039	32.543207
711.392769	40831.600963	32.548224
712.857785	40877.068680	32.553242
713.312990	40957.334229	32.558260
713.953358	41008.311128	32.563277
714.557368	41082.359145	32.568295
715.239041	41152.055196	32.573312
716.021111	41217.442919	32.578330
716.893480	41290.130725	32.583348
717.410510	41359.270337	32.588365
718.228734	41440.108003	32.593383
718.874906	41502.039518	32.598400
719.872316	41568.829402	32.603418
720.136949	41638.571754	32.608436
721.281983	41708.344535	32.613453
721.766447	41778.818905	32.618471
722.653398	41849.182168	32.623488
723.685723	41909.924492	32.628506
724.301291	41982.548880	32.633524
725.288067	42037.186138	32.638541
726.073056	42114.263036	32.643559
726.670727	42177.068957	32.648576
727.575880	42233.457800	32.653594
727.973194	42311.603499	32.658612
728.882108	42374.628696	32.663629
729.583749	42441.292430	32.668647
730.465318	42503.884013	32.673664
731.512216	42569.745716	32.678682
731.736275	42632.022933	32.683700
732.760749	42692.457001	32.688717
733.895303	42761.040253	32.693735
734.430768	42823.303278	32.698752
735.301203	42875.715854	32.703770
735.726014	42941.804197	32.708788
736.953025	42993.532647	32.713805
737.204119	43064.140910	32.718823
738.011489	43132.061691	32.723840
738.740623	43190.412172	32.728858
739.244814	43258.208228	32.733876
739.949709	43323.729811	32.738893
740.802107	43385.051705	32.743911
740.935253	43458.216508	32.748928
741.760185	43524.205522	32.753946
742.498474	43605.678048	32.758964
743.394371	43684.892497	32.763981
743.788276	43746.112017	32.768999
744.657755	43824.713032	32.774016
745.912206	43894.133415	32.779034
746.161941	43963.136758	32.784052
747.128101	44017.244157	32.789069
748.075413	44081.439809	32.794087
748.930082	44133.246730	32.799104
749.536728	44202.339311	32.804122
749.938651	44263.761275	32.809140
751.110423	44331.635060	32.814157
751.824824	44396.411550	32.819175
752.046187	44456.676811	32.824192
753.199163	44523.491235	32.829210
753.630714	44586.859183	32.834228
754.315268	44648.830584	32.839245
755.114911	44717.544322	32.844263
755.667723	44805.414966	32.849280
756.527331	44869.532857	32.854298
757.372076	44942.625323	32.859316
758.002016	45001.130192	32.864333
758.740395	45090.010629	32.869351
759.755494	45171.149887	32.874368
761.119536	45231.235912	32.879386
761.470823	45290.584268	32.884404
762.080148	45370.498757	32.889421
762.973454	45440.304610	32.894439
763.676526	45505.102805	32.899456
764.673829	45593.553393	32.904474
765.171119	45667.044933	32.909492
766.043804	45733.627849	32.914509
766.719837	45809.848869	32.919527
767.344191	45876.891461	32.924544
768.364413	45946.682290	32.929562
769.255878	46026.741002	32.934580
770.039892	46098.336784	32.939597
770.641105	46165.964672	32.944615
771.573018	46238.982440	32.949632
772.183611	46314.591399	32.954650
772.986413	46392.252362	32.959668
773.987413	46464.127438	32.964685
774.961883	46534.315959	32.969703
775.181650	46611.859327	32.974720
776.355383	46669.731089	32.979738
777.038521	46752.526977	32.984756
777.427596	46832.328606	32.989773
778.608354	46903.003190	32.994791
779.128721	46981.052468	32.999808
779.923097	47055.531088	33.004826
780.436260	47135.879101	33.009844
781.115185	47217.699770	33.014861
782.165402	47287.812988	33.019879
782.831576	47384.039610	33.024896
784.269650	47440.786468	33.029914
785.314541	47510.383979	33.034932
786.110321	47588.956884	33.039949
786.939053	47648.420214	33.044967
787.529011	47718.444350	33.049984
788.868533	47779.170926	33.055002
789.417279	47830.311821	33.060020
790.119928	47886.123349	33.065037
791.127804	47936.702403	33.070055
791.501397	47996.898810	33.075072
792.416126	48046.896666	33.080090
792.611068	48116.508821	33.085108
793.502953	48183.877331	33.090125
794.393530	48253.237299	33.095143
794.931527	48313.307643	33.100160
795.686435	48383.655244	33.105178
795.925546	48457.836924	33.110196
796.840310	48531.248737	33.115213
797.747123	48614.251260	33.120231
797.980867	48686.711926	33.125248
798.827456	48764.843379	33.130266
800.113878	48850.746337	33.135284
800.740578	48947.776610	33.140301
801.837537	49026.203836	33.145319
802.421784	49097.597491	33.150336
803.464458	49183.111721	33.155354
804.175789	49262.869876	33.160372
804.546069	49336.778756	33.165389
805.972392	49412.940110	33.170407
806.520718	49507.975865	33.175424
807.534613	49582.916149	33.180442
808.470234	49658.137430	33.185460
808.779678	49751.521138	33.190477
809.680084	49819.718116	33.195495
810.749612	49911.479618	33.200512
811.611507	49985.044710	33.205530
812.622478	50059.548839	33.210548
813.277783	50149.086524	33.215565
814.897842	50231.392970	33.220583
815.372753	50298.438277	33.225600
816.086384	50366.805930	33.230618
817.147615	50446.570495	33.235636
817.897580	50528.931614	33.240653
819.078996	50591.801022	33.245671
819.853853	50664.817902	33.250688
820.380186	50734.722059	33.255706
821.314637	50807.553177	33.260724
822.219635	50884.955669	33.265741
822.837362	50951.384254	33.270759
823.329188	51035.994685	33.275776
824.503336	51101.940787	33.280794
825.260418	51179.753107	33.285812
825.678042	51262.161035	33.290829
826.431958	51340.466866	33.295847
827.217747	51423.495440	33.300864
828.345847	51504.409127	33.305882
829.175313	51586.617289	33.310900
830.109541	51675.913087	33.315917
831.087458	51750.186525	33.320935
831.633602	51827.751200	33.325952
832.468584	51892.390838	33.330970
833.174180	51971.852722	33.335988
833.989967	52038.468413	33.341005
835.085343	52111.115107	33.346023
835.729857	52186.371275	33.351040
836.410584	52251.147217	33.356058
837.478085	52328.460643	33.361076
837.974723	52406.490159	33.366093
839.176754	52467.387200	33.371111
839.774590	52556.071833	33.376128
840.767796	52621.474768	33.381146
841.609055	52694.574555	33.386164
842.008465	52770.149909	33.391181
842.950571	52856.291064	33.396199
843.725823	52943.118817	33.401216
844.782812	53013.029434	33.406234
845.590258	53096.100153	33.411252
845.875867	53185.689735	33.416269
847.502558	53253.661094	33.421287
847.955237	53342.262225	33.426304
848.745051	53429.269899	33.431322
849.672055	53508.163600	33.436340
850.790466	53596.057173	33.441357
851.978267	53683.633972	33.446375
852.495169	53771.128602	33.451392
853.596716	53838.374588	33.456410
854.268742	53928.199870	33.461428
855.392524	54003.087477	33.466445
856.327870	54083.598387	33.471463
856.718011	54165.897696	33.476480
857.336403	54249.467777	33.481498
858.711817	54329.701418	33.486516
859.459035	54420.318883	33.491533
860.384875	54501.101450	33.496551
861.317658	54591.103143	33.501568
862.466612	54666.791211	33.506586
863.369907	54733.058856	33.511604
863.851029	54835.999278	33.516621
864.990573	54909.950651	33.521639
865.906144	54989.708014	33.526656
866.574733	55069.432437	33.531674
867.708400	55153.559114	33.536692
868.517112	55231.244934	33.541709
869.437499	55300.662133	33.546727
870.250908	55394.679810	33.551744
871.204499	55471.150418	33.556762
871.983957	55545.101704	33.561780
872.524074	55641.951404	33.566797
873.717241	55711.853904	33.571815
874.517494	55799.950814	33.576832
875.314162	55884.238663	33.581850
876.212251	55965.319387	33.586868
876.846714	56048.124929	33.591885
877.757201	56138.803858	33.596903
878.375569	56223.194247	33.601920
879.346106	56309.233596	33.606938
880.466339	56375.046521	33.611956
881.193423	56473.562860	33.616973
882.235811	56541.418552	33.621991
882.901745	56611.121134	33.627008
883.638964	56678.887006	33.632026
884.805828	56769.070517	33.637044
885.382923	56854.385843	33.642061
886.470393	56931.071687	33.647079
887.132328	57019.202779	33.652096
887.878788	57099.523440	33.657114
889.077110	57174.787864	33.662132
889.553259	57266.930504	33.667149
890.445817	57351.001471	33.672167
891.428391	57450.401033	33.677184
892.054360	57538.183600	33.682202
893.173562	57618.683972	33.687220
894.290987	57720.393343	33.692237
895.053041	57812.922552	33.697255
896.152147	57905.411211	33.702272
897.191326	57975.855116	33.707290
897.940349	58067.188015	33.712308
898.610019	58167.749345	33.717325
899.722619	58244.774458	33.722343
900.795215	58331.239528	33.727360
901.593282	58432.173334	33.732378
903.055935	58509.257495	33.737396
903.922453	58599.630355	33.742413
904.464582	58678.857003	33.747431
905.408334	58765.092034	33.752448
906.046572	58848.582017	33.757466
907.694101	58941.061191	33.762484
908.150989	59026.730858	33.767501
909.133154	59099.830666	33.772519
910.291995	59197.604556	33.777536
911.127606	59289.861070	33.782554
911.947608	59373.084536	33.787572
912.595695	59455.893718	33.792589
913.556630	59542.710557	33.797607
914.792595	59638.419116	33.802624
915.788889	59734.602014	33.807642
916.560869	59810.450176	33.812660
917.224562	59907.892986	33.817677
918.186877	59996.991307	33.822695
919.265586	60086.159937	33.827712
919.989468	60176.935725	33.832730
920.948304	60275.656422	33.837748
921.650337	60374.879487	33.842765
922.629020	60461.438871	33.847783
923.990277	60545.102406	33.852800
924.677638	60651.777645	33.857818
925.640940	60723.434400	33.862836
926.306361	60825.122178	33.867853
927.262817	60918.273704	33.872871
928.477088	61004.498149	33.877888
929.168017	61113.212035	33.882906
930.615596	61175.380885	33.887924
931.507204	61274.922719	33.892941
931.887548	61349.017534	33.897959
932.844710	61426.977293	33.902976
933.493294	61514.140329	33.907994
934.780075	61585.597340	33.913012
935.442884	61682.067502	33.918029
936.162990	61778.715341	33.923047
937.204097	61860.938978	33.928064
938.031065	61961.022056	33.933082
939.050142	62056.906958	33.938100
939.785443	62141.668735	33.943117
940.663359	62242.935653	33.948135
941.770141	62337.374424	33.953152
942.586605	62434.913402	33.958170
943.510428	62541.921713	33.963188
944.318223	62645.210282	33.968205
945.017626	62749.246114	33.973223
946.388136	62850.112650	33.978240
947.178955	62956.942372	33.983258
948.035240	63060.834955	33.988276
948.794073	63169.256204	33.993293
950.348677	63275.063034	33.998311
951.076234	63387.706283	34.003328
951.801435	63495.288428	34.008346
953.462044	63586.149490	34.013364
954.514076	63691.530188	34.018381
955.301639	63795.355620	34.023399
956.428455	63899.746603	34.028416
957.363078	63988.704001	34.033434
958.482782	64079.836660	34.038452
959.351619	64178.408943	34.043469
960.424762	64269.777299	34.048487
961.913648	64376.655516	34.053504
962.121307	64477.459930	34.058522
963.228679	64567.598932	34.063540
964.290465	64667.586294	34.068557
965.080598	64769.468069	34.073575
966.597951	64873.407480	34.078592
967.325128	64973.822349	34.083610
968.167571	65064.969094	34.088628
969.202807	65158.353181	34.093645
970.283196	65261.088319	34.098663
971.230811	65364.460989	34.103680
971.813621	65467.680659	34.108698
973.240026	65554.659525	34.113716
973.918712	65663.196136	34.118733
974.871348	65759.621928	34.123751
976.241523	65860.267595	34.128768
977.044394	65955.928625	34.133786
978.043305	66054.480406	34.138804
978.867537	66160.991123	34.143821
979.838909	66265.498717	34.148839
981.021379	66358.732571	34.153856
981.876565	66464.043010	34.158874
982.814778	66547.241318	34.163892
983.950783	66638.099310	34.168909
984.709852	66723.679920	34.173927
985.568874	66820.748141	34.178944
986.173309	66914.146140	34.183962
987.236057	66992.617259	34.188980
988.030313	67100.208666	34.193997
989.168013	67191.656479	34.199015
990.390640	67299.477741	34.204032
990.965432	67415.608627	34.209050
991.694874	67498.007230	34.214068
992.782473	67612.958524	34.219085
993.782440	67713.811754	34.224103
994.664840	67828.019953	34.229120
995.779411	67934.238405	34.234138
997.010985	68048.973542	34.239156
997.824318	68160.471914	34.244173
998.398644	68269.343007	34.249191
999.819501	68371.983694	34.254208
1000.540965	68500.498871	34.259226
1001.952218	68605.385025	34.264244
1002.842589	68720.570097	34.269261
1003.874360	68844.344231	34.274279
1004.802843	68945.013062	34.279296
1005.961799	69068.686255	34.284314
1006.664860	69176.998617	34.289332
1007.934193	69292.095184	34.294349
1008.925093	69405.025506	34.299367
1010.366125	69519.874977	34.304384
1011.124622	69632.502426	34.309402
1012.252917	69737.294377	34.314420
1013.535334	69857.345410	34.319437
1014.221658	69971.951167	34.324455
1015.420807	70070.049229	34.329472
1016.756568	70193.897267	34.334490
1017.890003	70304.560883	34.339508
1018.909832	70403.415720	34.344525
1020.146477	70515.144498	34.349543
1021.534956	70611.667208	34.354560
1022.384094	70714.853437	34.359578
1023.469991	70813.668236	34.364596
1024.717761	70909.229150	34.369613
1025.304363	71013.286403	34.374631
1026.751036	71118.028757	34.379648
1027.460285	71222.092873	34.384666
1028.454176	71307.277140	34.389684
1029.244387	71416.478884	34.394701
1030.237158	71530.545810	34.399719
1031.589150	71623.256620	34.404736
1032.283912	71733.265111	34.409754
1033.223515	71847.051670	34.414772
1034.243129	71955.069916	34.419789
1035.296364	72071.430310	34.424807
1036.321225	72171.525345	34.429824
1037.390669	72267.058017	34.434842
1038.250470	72369.695150	34.439860
1039.580089	72466.185750	34.444877
1040.109340	72570.816367	34.449895
1041.559366	72653.456904	34.454912
1042.543183	72776.922190	34.459930
1043.153228	72864.120429	34.464948
1044.326574	72953.586391	34.469965
1045.268022	73065.338636	34.474983
1046.837477	73160.372695	34.480000
1047.915923	73259.693776	34.485018
1049.100623	73358.575075	34.490036
1050.033693	73457.762295	34.495053
1051.458366	73540.707554	34.500071
1052.465075	73619.732284	34.505088
1053.350193	73734.189187	34.510106
1054.495856	73824.990492	34.515124
1055.722884	73904.910224	34.520141
1056.652505	74008.783267	34.525159
1057.554500	74112.534858	34.530176
1058.619769	74218.997274	34.535194
1059.353720	74314.947024	34.540212
1060.582555	74424.929665	34.545229
1061.101781	74542.425819	34.550247
1062.475181	74643.969213	34.555264
1063.578245	74758.687996	34.560282
1064.033427	74883.084563	34.565300
1065.771484	74983.617421	34.570317
1066.436750	75094.780345	34.575335
1067.594954	75206.288884	34.580352
1068.393950	75329.748772	34.585370
1069.459063	75444.003528	34.590388
1070.402652	75570.102479	34.595405
1071.524438	75691.149653	34.600423
1073.000063	75796.695663	34.605440
1074.276567	75932.855612	34.610458
1074.908748	76049.754843	34.615476
1076.313785	76158.562394	34.620493
1077.604724	76289.578039	34.625511
1078.557961	76390.040523	34.630528
1079.351246	76517.945213	34.635546
1080.702273	76630.227269	34.640564
1081.880514	76736.906226	34.645581
1082.580368	76867.444502	34.650599
1083.752086	76974.770401	34.655616
1085.333042	77100.057001	34.660634
1086.227915	77218.633960	34.665652
1088.028225	77311.167085	34.670669
1088.886111	77433.315815	34.675687
1089.919320	77533.802841	34.680704
1091.142213	77650.168582	34.685722
1092.102951	77762.898205	34.690740
1093.498605	77859.043944	34.695757
1094.067016	77978.220811	34.700775
1095.431159	78075.200565	34.705792
1096.513335	78179.405767	34.710810
1097.743861	78283.689033	34.715828
1098.988381	78381.612076	34.720845
1099.725695	78472.227442	34.725863
1100.921106	78564.287303	34.730880
1101.921893	78672.666961	34.735898
1103.001171	78758.495002	34.740916
1104.218479	78853.871063	34.745933
1104.741686	78964.407754	34.750951
1105.759925	79069.866533	34.755968
1106.833431	79178.698719	34.760986
1107.669847	79292.196080	34.766004
1108.920048	79399.579133	34.771021
1110.040491	79512.084394	34.776039
1111.061562	79636.792944	34.781056
1112.170905	79750.085075	34.786074
1113.128491	79856.726927	34.791092
1114.558002	79990.272705	34.796109
1115.387320	80107.195401	34.801127
1116.618169	80223.631376	34.806144
1117.892797	80344.182471	34.811162
1118.704281	80472.715813	34.816180
1120.041491	80579.408479	34.821197
1121.365652	80705.276320	34.826215
1122.515557	80820.887798	34.831232
1123.517738	80943.489588	34.836250
1124.710816	81060.441993	34.841268
1126.019841	81177.193293	34.846285
1127.126422	81317.120462	34.851303
1128.171909	81421.120330	34.856320
1129.476139	81540.251332	34.861338
1130.545124	81665.520785	34.866356
1131.551395	81794.385341	34.871373
1132.670718	81912.612280	34.876391
1133.892181	82033.649454	34.881408
1135.148070	82160.624310	34.886426
1136.166426	82279.887193	34.891444
1137.514591	82404.870137	34.896461
1138.676278	82534.991559	34.901479
1139.693035	82644.982596	34.906496
1140.705896	82757.800738	34.911514
1142.080717	82896.229150	34.916532
1143.676516	83020.556836	34.921549
1144.462734	83131.415279	34.926567
1145.685996	83252.996602	34.931584
1146.700701	83378.544160	34.936602
1147.989663	83503.189037	34.941620
1149.310710	83607.048486	34.946637
1150.305351	83727.821743	34.951655
1151.306062	83854.240514	34.956672
1152.723370	83965.553026	34.961690
1153.904293	84098.266905	34.966708
1154.822914	84207.598922	34.971725
1155.587526	84348.833603	34.976743
1156.882679	84463.006935	34.981760
1158.488948	84585.356961	34.986778
1159.279675	84703.746724	34.991796
1160.922924	84806.574531	34.996813
1161.821695	84918.872341	35.001831
1162.436518	85030.046219	35.006848
1163.501009	85140.940520	35.011866
1164.323890	85258.866717	35.016884
1165.773372	85376.662306	35.021901
1166.877712	85484.080888	35.026919
1167.884788	85614.663220	35.031936
1168.738164	85739.580248	35.036954
1170.086925	85872.860258	35.041972
1171.748341	85993.496148	35.046989
1172.832355	86126.231818	35.052007
1173.961501	86243.134711	35.057024
1175.282377	86371.161555	35.062042
1176.264563	86500.008120	35.067060
1177.754180	86627.048561	35.072077
1178.636836	86751.593797	35.077095
1180.020879	86882.882723	35.082112
1181.158495	87003.740413	35.087130
1181.703053	87135.619660	35.092148
1183.325789	87273.069800	35.097165
1184.673155	87410.564613	35.102183
1185.831377	87540.445439	35.107200
1187.061620	87670.625443	35.112218
1188.210249	87802.096550	35.117236
1189.379135	87937.504766	35.122253
1190.847849	88081.624230	35.127271
1191.897340	88213.151554	35.132288
1193.330963	88340.634727	35.137306
1194.321647	88479.084717	35.142324
1195.552788	88599.999745	35.147341
1196.575984	88742.379577	35.152359
1197.841828	88881.218399	35.157376
1199.311209	89009.028669	35.162394
1200.528877	89146.106190	35.167412
1201.537316	89275.673471	35.172429
1202.860181	89418.452766	35.177447
1204.049322	89544.407259	35.182464
1205.011667	89688.839296	35.187482
1206.295739	89822.451308	35.192500
1207.897619	89953.667375	35.197517
1208.864764	90093.965399	35.202535
1210.078456	90236.596676	35.207552
1211.366039	90363.115754	35.212570
1212.817260	90492.721064	35.217588
1214.268656	90635.070505	35.222605
1215.504089	90760.917162	35.227623
1216.413352	90891.945447	35.232640
1217.704135	91018.663869	35.237658
1218.923807	91157.315852	35.242676
1220.453703	91289.032053	35.247693
1221.519544	91416.585427	35.252711
1222.550022	91554.454146	35.257728
1224.152516	91667.130575	35.262746
1225.113660	91798.174998	35.267764
1226.498743	91923.125414	35.272781
1227.159721	92034.758080	35.277799
1228.532775	92149.528983	35.282816
1229.944757	92258.513489	35.287834
1230.636141	92402.633353	35.292852
1231.859650	92522.066034	35.297869
1233.269703	92655.675298	35.302887
1234.274463	92778.869484	35.307904
1235.602316	92902.265981	35.312922
1236.787855	93041.586727	35.317940
1237.607266	93164.926383	35.322957
1239.068285	93309.840581	35.327975
1240.232691	93445.985739	35.332992
1241.643582	93574.141879	35.338010
1242.225265	93732.462405	35.343028
1243.860252	93856.896983	35.348045
1245.617731	94006.638988	35.353063
1246.554247	94149.289074	35.358080
1248.074387	94279.614130	35.363098
1249.322218	94437.289772	35.368116
1250.581835	94558.574678	35.373133
1251.899493	94705.728325	35.378151
1252.913229	94844.625923	35.383168
1254.730414	94978.930832	35.388186
1255.495082	95122.322911	35.393204
1256.578884	95270.137354	35.398221
1258.290795	95403.234384	35.403239
1259.553987	95548.928362	35.408256
1261.214434	95685.229710	35.413274
1262.520252	95818.956761	35.418292
1263.824201	95954.917904	35.423309
1265.324467	96097.123868	35.428327
1266.586494	96220.574489	35.433344
1267.981191	96353.936341	35.438362
1269.109707	96494.166979	35.443380
1270.112781	96624.701745	35.448397
1271.997308	96761.884926	35.453415
1273.095805	96889.515066	35.458432
1274.485528	97023.723028	35.463450
1275.837422	97162.695039	35.468468
1277.004863	97285.502277	35.473485
1278.261931	97415.412889	35.478503
1279.066470	97544.402974	35.483520
1280.776790	97672.958777	35.488538
1281.825330	97823.205849	35.493556
1282.991485	97951.761175	35.498573
1284.744262	98078.547476	35.503591
1285.783373	98220.865403	35.508608
1287.084683	98356.873021	35.513626
1288.381109	98488.548584	35.518644
1289.936235	98622.322142	35.523661
1291.082696	98749.904489	35.528679
1291.912005	98900.883106	35.533696
1293.381535	99022.753307	35.538714
1294.258971	99152.183756	35.543732
1295.522591	99266.869265	35.548749
1296.784376	99388.065847	35.553767
1297.949154	99526.968137	35.558784
1299.306834	99664.992807	35.563802
1300.611605	99800.306174	35.568820
1301.678907	99923.630686	35.573837
1302.951152	100060.627377	35.578855
1304.006467	100199.051300	35.583872
1305.532348	100330.416245	35.588890
1306.753505	100479.919360	35.593908
1308.062648	100627.909939	35.598925
1309.278825	100765.818174	35.603943
1310.689326	100908.764385	35.608960
1312.151586	101058.074730	35.613978
1313.371836	101193.586861	35.618996
1314.721656	101357.393708	35.624013
1315.978591	101492.427207	35.629031
1317.161204	101650.992057	35.634048
1318.815385	101781.876619	35.639066
1319.815826	101941.782180	35.644084
1321.232380	102089.973813	35.649101
1322.816988	102234.159670	35.654119
1323.986275	102387.030562	35.659136
1325.214915	102532.287255	35.664154
1326.746336	102698.972702	35.669172
1328.018401	102847.780582	35.674189
1329.681972	102992.502745	35.679207
1331.055273	103156.900644	35.684224
1332.490039	103292.549062	35.689242
1333.432745	103444.190984	35.694260
1335.071276	103609.638278	35.699277
1336.689736	103738.077925	35.704295
1337.789501	103890.672257	35.709312
1339.297980	104032.951255	35.714330
1340.836630	104195.140639	35.719348
1341.883729	104341.570096	35.724365
1343.331940	104476.223360	35.729383
1344.373130	104642.158865	35.734400
1346.088318	104785.130946	35.739418
1347.211994	104930.096386	35.744436
1348.698649	105085.813704	35.749453
1350.278625	105235.081314	35.754471
1351.643795	105384.921916	35.759488
1353.019470	105527.534770	35.764506
1353.948346	105688.622578	35.769524
1355.426685	105826.120183	35.774541
1357.068166	105987.546063	35.779559
1358.441583	106144.813483	35.784576
1359.774540	106274.900733	35.789594
1361.454153	106431.248023	35.794612
1362.504842	106568.798896	35.799629
1364.112335	106719.970030	35.804647
1365.169563	106872.406730	35.809664
1366.635150	107016.431820	35.814682
1367.911947	107144.469537	35.819700
1369.127042	107279.359234	35.824717
1370.500907	107405.205786	35.829735
1371.630133	107543.964908	35.834752
1373.085532	107686.210874	35.839770
1374.540212	107814.097302	35.844788
1375.352328	107967.890002	35.849805
1376.948009	108109.976931	35.854823
1378.359707	108256.011659	35.859840
1379.556972	108408.169992	35.864858
1380.913820	108557.500085	35.869876
1382.539305	108705.301033	35.874893
1383.692729	108857.709666	35.879911
1384.721501	109008.335216	35.884928
1386.508498	109162.214727	35.889946
1388.051846	109318.811268	35.894964
1389.377716	109476.221903	35.899981
1390.850988	109620.185327	35.904999
1392.110065	109797.122396	35.910016
1393.412958	109952.887755	35.915034
1395.073856	110103.001848	35.920052
1396.090561	110260.916078	35.925069
1398.066680	110402.766052	35.930087
1399.354258	110572.545345	35.935104
1400.529822	110730.658891	35.940122
1401.994186	110885.847499	35.945140
1403.426004	111052.606863	35.950157
1404.867225	111212.573906	35.955175
1406.106572	111373.814735	35.960192
1407.820031	111541.140316	35.965210
1409.307721	111702.603353	35.970228
1410.476210	111860.440422	35.975245
1412.377733	112016.592136	35.980263
1413.587327	112184.021139	35.985280
1415.133295	112343.358504	35.990298
1416.735093	112506.682379	35.995316
1417.873072	112661.319982	36.000333
1419.895264	112819.958027	36.005351
1421.054582	112986.894009	36.010368
1422.488142	113134.017788	36.015386
1424.215516	113297.326898	36.020404
1425.286992	113451.277298	36.025421
1426.979953	113614.150818	36.030439
1428.385677	113767.638564	36.035456
1429.602411	113921.397849	36.040474
1431.492354	114072.626468	36.045492
1432.403400	114253.005915	36.050509
1434.043971	114400.655013	36.055527
1435.377387	114561.021569	36.060544
1437.008887	114723.095397	36.065562
1438.121633	114879.099167	36.070580
1439.545786	115034.585931	36.075597
1441.336284	115190.559890	36.080615
1442.521496	115350.163658	36.085632
1443.986143	115511.262450	36.090650
1445.530084	115652.577953	36.095668
1446.947941	115791.103304	36.100685
1448.363604	115936.074787	36.105703
1449.523269	116088.039335	36.110720
1451.095179	116231.677138	36.115738
1452.274964	116377.353395	36.120756
1453.544259	116528.024252	36.125773
1455.052909	116684.590348	36.130791
1456.798498	116829.045980	36.135808
1457.643252	116983.193225	36.140826
1459.493182	117140.568947	36.145844
1460.782219	117304.182566	36.150861
1461.993120	117461.699801	36.155879
1463.763130	117619.477387	36.160896
1465.090912	117796.928625	36.165914
1466.719091	117949.766863	36.170932
1468.295410	118116.170219	36.175949
1469.685498	118275.487473	36.180967
1471.056963	118428.356686	36.185984
1472.667262	118601.589667	36.191002
1473.807334	118767.490363	36.196020
1475.248583	118945.406361	36.201037
1477.103933	119107.979021	36.206055
1478.726471	119283.234485	36.211072
1480.292998	119452.320065	36.216090
1481.698220	119617.411575	36.221108
1482.910640	119795.869995	36.226125
1484.727631	119941.154907	36.231143
1486.181885	120128.062129	36.236160
1488.070984	120299.843761	36.241178
1489.533473	120455.129332	36.246196
1491.171758	120628.460039	36.251213
1492.594608	120796.772983	36.256231
1494.223597	120958.848601	36.261248
1495.978333	121122.500991	36.266266
1497.170225	121301.302232	36.271284
1498.675965	121461.234863	36.276301
1500.208834	121619.125105	36.281319
1501.758150	121791.160479	36.286336
1502.978646	121958.309842	36.291354
1505.039941	122128.581614	36.296372
1506.269662	122301.013052	36.301389
1507.704111	122459.455901	36.306407
1508.973351	122645.789828	36.311424
1510.571444	122812.871929	36.316442
1512.520785	122972.021292	36.321460
1513.887159	123144.487165	36.326477
1515.239175	123315.803856	36.331495
1516.651581	123481.779751	36.336512
1518.241452	123652.794835	36.341530
1520.039646	123814.329107	36.346548
1521.420271	123992.599213	36.351565
1523.036737	124166.171900	36.356583
1524.466895	124322.739267	36.361600
1525.625378	124506.114567	36.366618
1527.028689	124657.545641	36.371636
1528.368318	124818.728174	36.376653
1530.112893	124960.708244	36.381671
1531.705048	125120.471815	36.386688
1532.574683	125290.421117	36.391706
1534.488960	125441.864088	36.396724
1535.785862	125613.368879	36.401741
1537.083303	125775.399841	36.406759
1538.415828	125950.612506	36.411776
1540.176511	126137.817309	36.416794
1541.773392	126298.676458	36.421812
1543.048087	126476.055113	36.426829
1544.753738	126653.771810	36.431847
1546.422446	126824.895836	36.436864
1547.800228	127023.428863	36.441882
1549.404518	127193.045336	36.446900
1551.180330	127384.221245	36.451917
1552.793503	127557.803538	36.456935
1554.298862	127742.906416	36.461952
1555.989996	127935.417074	36.466970
1557.781590	128108.404451	36.471988
1558.872410	128292.512780	36.477005
1560.794638	128464.138827	36.482023
1562.353709	128651.696903	36.487040
1563.584873	128838.332888	36.492058
1565.444512	129015.014288	36.497076
1566.977491	129215.540088	36.502093
1568.538266	129395.058456	36.507111
1569.915004	129602.997644	36.512128
1571.532093	129782.180182	36.517146
1573.523735	129953.703087	36.522164
1574.827335	130155.995069	36.527181
1576.742770	130348.828938	36.532199
1578.444725	130525.418299	36.537216
1580.269990	130710.502853	36.542234
1582.094034	130888.798117	36.547252
1583.693198	131076.784256	36.552269
1585.125162	131250.912557	36.557287
1586.859160	131426.869037	36.562304
1588.307820	131614.198526	36.567322
1590.278618	131784.849092	36.572340
1591.501495	131962.777889	36.577357
1592.959231	132147.600874	36.582375
1594.972833	132329.156625	36.587392
1596.349958	132522.090910	36.592410
1597.941044	132686.016136	36.597428
1599.454868	132892.006698	36.602445
1601.388493	133072.122844	36.607463
1602.590918	133244.006566	36.612480
1604.000023	133432.646721	36.617498
1606.108458	133614.030901	36.622516
1607.978526	133790.145148	36.627533
1609.463731	133980.157914	36.632551
1610.938375	134153.334274	36.637568
1612.531725	134337.060238	36.642586
1613.982129	134488.106650	36.647604
1615.250296	134657.314863	36.652621
1617.122858	134828.620143	36.657639
1618.732907	134983.445089	36.662656
1619.945528	135149.446567	36.667674
1621.504182	135318.321078	36.672692
1623.062134	135513.096770	36.677709
1624.642979	135686.861020	36.682727
1626.471213	135850.500557	36.687744
1627.346527	136033.388334	36.692762
1629.350159	136206.708393	36.697780
1630.790782	136398.923657	36.702797
1632.456032	136585.123443	36.707815
1634.013697	136774.965648	36.712832
1635.516457	136973.599441	36.717850
1637.295051	137157.491251	36.722868
1639.107468	137342.278560	36.727885
1640.683981	137544.630094	36.732903
1642.499543	137732.790154	36.737920
1644.280478	137935.618796	36.742938
1645.727992	138113.321715	36.747956
1647.226178	138324.688451	36.752973
1649.375017	138521.025052	36.757991
1651.101184	138709.598385	36.763008
1652.724660	138909.265203	36.768026
1654.675672	139089.732703	36.773044
1656.496527	139285.695582	36.778061
1657.847520	139477.108739	36.783079
1659.785154	139661.218974	36.788096
1661.232695	139865.216310	36.793114
1663.220920	140052.780692	36.798132
1665.092819	140245.421375	36.803149
1666.593167	140430.302827	36.808167
1668.683748	140610.567245	36.813184
1669.481138	140818.945279	36.818202
1671.754998	141010.082237	36.823220
1673.380935	141187.204801	36.828237
1675.031998	141393.296686	36.833255
1676.631600	141583.707890	36.838272
1678.340967	141777.220650	36.843290
1680.045302	141970.329874	36.848308
1681.272232	142172.666855	36.853325
1682.848904	142361.958582	36.858343
1685.182929	142569.027281	36.863360
1686.473526	142770.534288	36.868378
1688.745874	142960.707843	36.873396
1690.485946	143156.974837	36.878413
1691.948082	143349.966482	36.883431
1693.529956	143548.339738	36.888448
1695.153000	143732.765494	36.893466
1697.069329	143939.491521	36.898484
1698.709566	144133.309004	36.903501
1700.058750	144336.870304	36.908519
1701.961026	144529.013576	36.913536
1703.408532	144722.662556	36.918554
1705.123472	144912.024065	36.923572
1706.583948	145088.561694	36.928589
1708.268358	145279.565404	36.933607
1710.067811	145460.753880	36.938624
1711.419973	145637.032954	36.943642
1713.364763	145829.570446	36.948660
1714.844596	146022.233663	36.953677
1716.312585	146195.011670	36.958695
1718.094985	146398.492276	36.963712
1719.636809	146604.687023	36.968730
1721.538171	146803.017603	36.973748
1723.393188	146994.030014	36.978765
1724.647074	147214.547740	36.983783
1726.606523	147421.188544	36.988800
1728.151692	147634.893820	36.993818
1729.966986	147835.348808	36.998836
1731.687890	148053.478413	37.003853
1733.570019	148264.472342	37.008871
1735.137237	148467.252485	37.013888
1736.816271	148682.515433	37.018906
1738.612082	148897.165472	37.023924
1740.565050	149120.171438	37.028941
1742.086107	149337.162571	37.033959
1744.133560	149545.590601	37.038976
1745.768693	149766.103416	37.043994
1747.721349	149979.823010	37.049012
1749.577062	150201.419366	37.054029
1751.506410	150420.127765	37.059047
1753.460279	150625.319512	37.064064
1754.835802	150847.643078	37.069082
1756.777254	151071.108032	37.074100
1758.614083	151291.104742	37.079117
1760.291590	151506.690979	37.084135
1762.299133	151717.687527	37.089152
1763.931619	151933.892262	37.094170
1765.757688	152153.592193	37.099188
1767.717652	152367.896777	37.104205
1769.155162	152578.507586	37.109223
1771.815488	152792.830506	37.114240
1773.509580	153007.156095	37.119258
1775.271355	153215.209137	37.124276
1777.038070	153430.717709	37.129293
1778.799448	153644.415472	37.134311
1781.035302	153840.276339	37.139328
1782.310282	154055.841670	37.144346
1784.093991	154272.456036	37.149364
1786.116927	154477.483259	37.154381
1787.505921	154691.766675	37.159399
1789.537594	154895.438400	37.164416
1791.441367	155117.833522	37.169434
1793.066592	155337.560962	37.174452
1794.975359	155541.294138	37.179469
1796.563857	155755.882293	37.184487
1798.731703	155969.568330	37.189504
1800.282691	156170.268278	37.194522
1802.241461	156369.826890	37.199540
1804.417001	156550.890515	37.204557
1805.823537	156750.716549	37.209575
1807.471851	156918.361805	37.214592
1808.988665	157108.903415	37.219610
1810.668628	157308.778050	37.224628
1812.671808	157504.646335	37.229645
1814.097394	157706.186718	37.234663
1815.682035	157913.954396	37.239680
1817.462169	158116.848395	37.244698
1819.265349	158337.657352	37.249716
1821.476942	158538.456453	37.254733
1823.084966	158760.009186	37.259751
1824.992746	158956.002274	37.264768
1826.590305	159181.680558	37.269786
1828.323296	159399.717632	37.274804
1830.477596	159594.394403	37.279821
1832.462588	159822.031565	37.284839
1834.227112	160045.837486	37.289856
1836.449681	160255.255132	37.294874
1837.880898	160471.051480	37.299892
1839.843330	160686.460461	37.304909
1841.459950	160907.163047	37.309927
1843.278927	161131.284228	37.314944
1845.027158	161362.621149	37.319962
1846.856506	161584.777906	37.324980
1849.255120	161802.394409	37.329997
1850.862252	162028.342974	37.335015
1852.841313	162248.070553	37.340032
1855.032928	162475.070509	37.345050
1856.854620	162699.112311	37.350068
1858.882744	162913.611193	37.355085
1860.584681	163150.191996	37.360103
1862.773056	163376.094791	37.365120
1864.857612	163585.388989	37.370138
1866.598685	163806.292553	37.375156
1868.896962	164016.202106	37.380173
1870.442843	164227.855666	37.385191
1872.470765	164439.890505	37.390208
1874.843256	164669.247122	37.395226
1877.051406	164866.188817	37.400244
1878.954627	165079.667618	37.405261
1880.238376	165301.553276	37.410279
1882.003511	165497.515992	37.415296
1883.928680	165702.712948	37.420314
1885.470241	165917.471568	37.425332
1888.016224	166133.530558	37.430349
1889.769076	166362.564826	37.435367
1891.630303	166573.471519	37.440384
1893.231263	166780.412767	37.445402
1895.238308	166996.676458	37.450420
1897.436788	167216.272147	37.455437
1899.308810	167433.993031	37.460455
1900.658523	167638.302648	37.465472
1902.822838	167855.117081	37.470490
1904.698673	168049.781869	37.475508
1906.492437	168245.779809	37.480525
1908.173031	168444.853556	37.485543
1909.685819	168622.874160	37.490560
1911.614889	168827.161647	37.495578
1913.154847	169047.988691	37.500596
1915.227798	169255.008090	37.505613
1917.002060	169467.111679	37.510631
1918.563243	169685.097747	37.515648
1920.338975	169905.613251	37.520666
1922.469593	170113.706304	37.525684
1924.397099	170343.662858	37.530701
1926.286484	170566.155574	37.535719
1928.147117	170790.607576	37.540736
1930.160524	171015.493280	37.545754
1931.831395	171255.897500	37.550772
1933.870585	171481.593631	37.555789
1935.861056	171724.588475	37.560807
1937.788624	171960.364304	37.565824
1940.002407	172176.560961	37.570842
1942.044310	172414.515899	37.575860
1944.075877	172652.017240	37.580877
1945.965766	172889.745460	37.585895
1948.287830	173118.044637	37.590912
1950.195512	173350.673236	37.595930
1952.199780	173587.461431	37.600948
1954.369659	173812.122599	37.605965
1956.302283	174048.138380	37.610983
1958.256770	174279.673981	37.616000
1960.763307	174508.611492	37.621018
1962.159812	174735.709402	37.626036
1964.517393	174974.695123	37.631053
1966.532910	175209.715040	37.636071
1968.832963	175428.414772	37.641088
1970.888008	175656.504341	37.646106
1972.781698	175890.342331	37.651124
1975.064833	176108.731242	37.656141
1976.938999	176337.424206	37.661159
1979.001965	176566.773556	37.666176
1981.294219	176795.148988	37.671194
1982.949471	177018.615534	37.676212
1985.481055	177229.003732	37.681229
1987.605832	177451.979446	37.686247
1989.345043	177675.854879	37.691264
1991.254734	177884.632365	37.696282
1992.973140	178100.304926	37.701300
1995.183639	178322.954525	37.706317
1996.965113	178548.261569	37.711335
1998.944821	178772.409201	37.716352
2001.352755	178989.017263	37.721370
2002.893342	179207.502244	37.726388
2004.878084	179426.032057	37.731405
2007.143381	179667.977631	37.736423
2009.209904	179875.281047	37.741440
2010.975767	180087.847791	37.746458
2012.863014	180292.568038	37.751476
2015.038245	180492.054286	37.756493
2016.743570	180692.592990	37.761511
2018.504456	180894.202280	37.766528
2020.827279	181096.015168	37.771546
2022.362208	181301.671600	37.776564
2024.642541	181508.872861	37.781581
2026.493188	181721.459607	37.786599
2028.140993	181939.091400	37.791616
2029.854057	182151.816274	37.796634
2032.369848	182379.463110	37.801652
2034.455996	182575.077801	37.806669
2036.267147	182809.779208	37.811687
2038.135164	183033.015155	37.816704
2040.614940	183247.666536	37.821722
2042.650491	183480.952864	37.826740
2044.533937	183718.908608	37.831757
2046.745657	183936.105532	37.836775
2048.723370	184157.007708	37.841792
2051.310681	184389.475312	37.846810
2053.608665	184611.788141	37.851828
2055.741106	184826.768732	37.856845
2057.997297	185038.482323	37.861863
2060.025336	185251.222861	37.866880
2062.497391	185464.528411	37.871898
2064.689910	185675.823668	37.876916
2067.286337	185886.256401	37.881933
2069.456015	186089.347248	37.886951
2071.271431	186300.933654	37.891968
2073.663439	186507.036542	37.896986
2075.586861	186716.247498	37.902004
2077.898692	186914.510139	37.907021
2079.813005	187122.062057	37.912039
2081.878356	187331.697434	37.917056
2083.892283	187527.192871	37.922074
2085.868071	187737.580303	37.927092
2088.072858	187950.812952	37.932109
2090.076806	188162.822143	37.937127
2092.286621	188364.190831	37.942144
2094.769153	188571.900198	37.947162
2096.789635	188792.627665	37.952180
2098.776777	188983.628487	37.957197
2101.195592	189176.033660	37.962215
2103.261184	189386.452335	37.967232
2105.377689	189596.343567	37.972250
2107.431046	189804.240673	37.977268
2109.516722	189992.476137	37.982285
2111.332277	190203.483789	37.987303
2113.436878	190409.827175	37.992320
2115.916997	190606.873151	37.997338
2118.171203	190823.829276	38.002356
2120.197314	191015.428539	38.007373
2122.396440	191220.707091	38.012391
2124.054879	191426.021527	38.017408
2126.287084	191627.349728	38.022426
2128.188833	191802.131116	38.027444
2130.571181	191990.238501	38.032461
2131.930464	192172.721828	38.037479
2133.969549	192346.861527	38.042496
2136.448799	192543.331740	38.047514
2137.937457	192742.815383	38.052532
2140.043982	192936.947677	38.057549
2142.196233	193130.959262	38.062567
2144.040056	193334.716661	38.067584
2146.437452	193540.938039	38.072602
2148.089008	193749.068069	38.077620
2150.004145	193966.942245	38.082637
2152.247790	194175.906607	38.087655
2154.174939	194409.924369	38.092672
2156.638883	194620.835520	38.097690
2158.463973	194853.919668	38.102708
2160.593008	195066.142281	38.107725
2163.281767	195300.271815	38.112743
2165.157445	195536.562094	38.117760
2167.379228	195751.653903	38.122778
2169.666462	195991.561651	38.127796
2171.881888	196225.123224	38.132813
2174.357120	196449.963290	38.137831
2176.489898	196689.302269	38.142848
2179.213586	196908.380786	38.147866
2181.343990	197133.380061	38.152884
2183.351885	197362.194729	38.157901
2186.082556	197592.710760	38.162919
2188.212384	197816.266148	38.167936
2190.787934	198030.968631	38.172954
2192.678335	198248.065312	38.177972
2195.206108	198473.007318	38.182989
2197.319548	198687.988855	38.188007
2199.539429	198907.434882	38.193024
2202.051033	199125.312423	38.198042
2204.046334	199350.659920	38.203060
2206.329188	199571.418738	38.208077
2208.701103	199783.748981	38.213095
2210.641097	200013.944011	38.218112
2213.189734	200230.233556	38.223130
2215.251870	200462.353145	38.228148
2217.838708	200673.853141	38.233165
2220.175371	200896.931670	38.238183
2222.154927	201124.142253	38.243200
2224.611074	201333.888494	38.248218
2226.407882	201547.154593	38.253236
2228.542416	201767.717378	38.258253
2231.183570	201991.399421	38.263271
2233.254546	202209.943112	38.268288
2235.587300	202433.142725	38.273306
2237.815206	202654.519301	38.278324
2239.997305	202873.708033	38.283341
2242.600600	203081.584288	38.288359
2244.296476	203314.827513	38.293376
2246.879641	203526.542088	38.298394
2248.482056	203719.537388	38.303412
2250.581284	203922.495344	38.308429
2252.876133	204118.860286	38.313447
2254.543615	204324.921972	38.318464
2256.748800	204534.491507	38.323482
2258.960759	204741.953533	38.328500
2260.937985	204951.801926	38.333517
2263.298245	205178.333813	38.338535
2265.009242	205401.554830	38.343552
2267.364238	205621.843777	38.348570
2269.591778	205865.803093	38.353588
2271.220257	206085.180768	38.358605
2274.336746	206316.027450	38.363623
2276.347244	206566.193531	38.368640
2278.823783	206805.191841	38.373658
2280.903356	207056.136091	38.378676
2283.149013	207292.951443	38.383693
2285.582064	207543.816300	38.388711
2287.672450	207799.116192	38.393728
2290.265426	208038.418337	38.398746
2292.446374	208286.888889	38.403764
2294.662567	208548.709784	38.408781
2297.248686	208791.760952	38.413799
2299.437381	209049.868770	38.418816
2301.785233	209300.018097	38.423834
2303.982519	209562.684189	38.428852
2306.683162	209801.430282	38.433869
2309.032049	210072.656349	38.438887
2310.987868	210321.107342	38.443904
2313.810537	210580.911027	38.448922
2316.243824	210827.320561	38.453940
2318.679943	211096.315554	38.458957
2320.908301	211344.143387	38.463975
2323.109401	211607.147517	38.468992
2325.497021	211851.321183	38.474010
2328.012935	212126.871426	38.479028
2330.627329	212384.214494	38.484045
2332.740558	212629.729568	38.489063
2334.802695	212890.361505	38.494080
2337.217690	213153.871245	38.499098
2340.085686	213411.965306	38.504116
2342.222527	213671.826765	38.509133
2345.029107	213920.258352	38.514151
2347.175998	214172.502672	38.519168
2349.441581	214430.785099	38.524186
2351.887041	214689.712893	38.529204
2354.214704	214945.105468	38.534221
2356.844567	215204.767773	38.539239
2359.115345	215458.558905	38.544256
2361.514704	215719.643608	38.549274
2363.846810	215975.432943	38.554292
2366.090546	216236.087225	38.559309
2368.495455	216482.103457	38.564327
2370.588030	216755.505397	38.569344
2373.024357	217000.198062	38.574362
2374.798350	217233.150784	38.579380
2376.810841	217478.369391	38.584397
2379.364872	217715.796187	38.589415
2381.523857	217963.697625	38.594432
2383.824440	218214.167598	38.599450
2386.056697	218455.952050	38.604468
2388.134431	218730.455914	38.609485
2390.710239	218978.891543	38.614503
2392.935934	219239.534396	38.619520
2394.986655	219498.377575	38.624538
2397.362040	219761.258611	38.629556
2399.592573	220050.306610	38.634573
2402.045022	220311.336338	38.639591
2404.266281	220603.333679	38.644608
2406.722031	220875.093887	38.649626
2409.177920	221161.063181	38.654644
2411.421813	221450.774754	38.659661
2414.156817	221741.323787	38.664679
2416.619881	222035.358010	38.669696
2419.184680	222327.548819	38.674714
2421.794362	222617.321118	38.679732
2424.226612	222907.109935	38.684749
2427.102897	223191.153664	38.689767
2429.281862	223491.130103	38.694784
2431.795410	223829.541055	38.699802
2434.287259	224124.784894	38.704820
2436.522726	224417.962654	38.709837
2439.075549	224700.209222	38.714855
2441.626204	225000.792720	38.719872
2444.273357	225287.534105	38.724890
2446.660551	225586.342592	38.729908
2449.234375	225888.246275	38.734925
2452.264892	226180.961536	38.739943
2454.591407	226479.579716	38.744960
2457.111704	226762.981376	38.749978
2459.813546	227060.958030	38.754996
2461.962951	227339.188806	38.760013
2464.709629	227637.414347	38.765031
2467.209466	227927.781759	38.770048
2469.928165	228216.769446	38.775066
2472.256136	228502.442280	38.780084
2474.892172	228797.006864	38.785101
2477.240965	229073.738629	38.790119
2479.216686	229367.165344	38.795136
2481.598861	229670.839772	38.800154
2484.696065	229971.659022	38.805172
2486.996285	230263.589622	38.810189
2489.326707	230562.881567	38.815207
2492.025573	230858.916042	38.820224
2494.451319	231159.363110	38.825242
2497.094705	231449.109733	38.830260
2499.159904	231752.892143	38.835277
2501.937887	232043.609788	38.840295
2504.404806	232338.771432	38.845312
2506.847364	232627.842393	38.850330
2509.287790	232905.231560	38.855348
2511.595731	233178.655053	38.860365
2513.872142	233448.096834	38.865383
2516.321675	233717.511925	38.870400
2518.831671	233989.661172	38.875418
2521.475601	234264.990119	38.880436
2523.528981	234551.080694	38.885453
2526.131143	234839.269373	38.890471
2528.311581	235122.776211	38.895488
2530.590551	235414.395740	38.900506
2533.033405	235710.028502	38.905524
2535.505791	236025.925541	38.910541
2537.924342	236316.687354	38.915559
2540.390352	236634.898535	38.920576
2543.057085	236950.665977	38.925594
2545.772987	237250.095055	38.930612
2547.780551	237567.492721	38.935629
2550.954939	237884.935003	38.940647
2553.556654	238197.135143	38.945664
2555.893280	238523.246156	38.950682
2558.720318	238844.556145	38.955700
2561.128131	239171.622952	38.960717
2563.723138	239498.051457	38.965735
2566.396905	239832.012075	38.970752
2569.078511	240144.814566	38.975770
2572.145263	240468.123127	38.980788
2573.943204	240807.102077	38.985805
2576.833024	241128.840312	38.990823
2579.453637	241459.435829	38.995840
2582.027720	241798.777207	39.000858
2584.785328	242123.104447	39.005876
2587.300688	242470.381799	39.010893
2590.282606	242792.338449	39.015911
2593.061938	243128.374344	39.020928
2595.573325	243460.059341	39.025946
2598.409718	243786.029424	39.030964
2600.894949	244125.645190	39.035981
2603.941152	244448.764248	39.040999
2606.325288	244779.913969	39.046016
2608.678274	245108.351583	39.051034
2611.910795	245439.343107	39.056052
2614.780793	245758.683146	39.061069
2617.252885	246087.459858	39.066087
2619.974289	246415.943836	39.071104
2622.355389	246735.287375	39.076122
2625.207981	247058.240063	39.081140
2627.853714	247388.541740	39.086157
2630.592677	247711.386883	39.091175
2633.271229	248040.871995	39.096192
2635.857561	248359.576948	39.101210
2638.441557	248685.649299	39.106228
2640.909245	249001.808873	39.111245
2643.668402	249335.729246	39.116263
2646.571624	249658.933523	39.121280
2649.132985	249970.888984	39.126298
2651.603152	250265.484886	39.131316
2653.936218	250569.145986	39.136333
2656.521416	250843.962321	39.141351
2659.096098	251139.787909	39.146368
2661.487507	251447.759643	39.151386
2664.091687	251745.918568	39.156404
2666.299430	252054.809548	39.161421
2668.909964	252370.368736	39.166439
2671.700506	252683.283578	39.171456
2673.885793	253001.400629	39.176474
2676.870882	253320.991850	39.181492
2679.316661	253662.108323	39.186509
2682.139999	253991.937911	39.191527
2684.594529	254324.950949	39.196544
2687.295597	254666.435206	39.201562
2690.016210	254994.021985	39.206580
2692.588843	255342.741959	39.211597
2695.060871	255677.685055	39.216615
2697.865307	256033.558311	39.221632
2700.335028	256384.658749	39.226650
2703.346945	256736.435940	39.231668
2705.620352	257107.560298	39.236685
2708.434117	257457.160016	39.241703
2711.697046	257808.416487	39.246720
2714.242217	258181.912777	39.251738
2717.006161	258540.387492	39.256756
2719.947558	258907.700131	39.261773
2722.685456	259271.438376	39.266791
2725.547715	259633.176035	39.271808
2728.112232	260002.175727	39.276826
2731.396775	260352.086038	39.281844
2734.023832	260721.559463	39.286861
2736.653702	261084.351995	39.291879
2739.445574	261459.414295	39.296896
2741.776789	261827.132405	39.301914
2744.957156	262195.961202	39.306932
2747.846447	262563.159950	39.311949
2750.610933	262932.563543	39.316967
2753.456001	263301.294310	39.321984
2756.362550	263674.537474	39.327002
2759.397806	264039.250637	39.332020
2762.366929	264404.203271	39.337037
2764.716219	264770.829427	39.342055
2768.036981	265131.713380	39.347072
2770.715227	265507.357029	39.352090
2773.094753	265865.316932	39.357108
2776.201120	266242.366808	39.362125
2778.971777	266608.368979	39.367143
2781.983406	266973.418756	39.372160
2784.496082	267345.152669	39.377178
2787.406773	267703.817355	39.382196
2790.235310	268077.584830	39.387213
2793.165541	268446.255792	39.392231
2796.048452	268804.773162	39.397248
2798.634797	269166.665539	39.402266
2801.351428	269496.402283	39.407284
2803.910527	269819.660880	39.412301
2806.347850	270152.947820	39.417319
2809.115909	270490.729722	39.422336
2811.675873	270836.064110	39.427354
2814.518889	271174.952155	39.432372
2817.162218	271531.171641	39.437389
2819.429290	271881.277808	39.442407
2822.676565	272233.642172	39.447424
2824.911532	272596.252092	39.452442
2827.804245	272955.404689	39.457460
2830.528743	273335.491005	39.462477
2833.172723	273701.872300	39.467495
2835.909814	274081.829731	39.472512
2838.310915	274474.694542	39.477530
2841.295244	274857.585096	39.482548
2844.402326	275246.095788	39.487565
2846.794568	275656.388799	39.492583
2850.112652	276048.346338	39.497600
2852.829798	276456.580986	39.502618
2855.552264	276848.708982	39.507636
2858.406763	277263.069398	39.512653
2861.282392	277662.412976	39.517671
2864.510670	278070.210759	39.522688
2867.293530	278490.145570	39.527706
2870.722415	278890.925415	39.532724
2873.599182	279311.505559	39.537741
2876.545652	279719.220395	39.542759
2879.771900	280120.666931	39.547776
2882.579505	280527.412654	39.552794
2885.841747	280935.280134	39.557812
2889.030768	281337.773480	39.562829
2891.992461	281732.986435	39.567847
2895.349064	282128.466859	39.572864
2897.651929	282540.448158	39.577882
2900.842122	282935.979786	39.582900
2903.893429	283336.080288	39.587917
2906.833346	283728.500945	39.592935
2909.668283	284134.198363	39.597952
2912.543089	284542.200800	39.602970
2915.481510	284934.061802	39.607988
2918.403856	285344.748688	39.613005
2921.309086	285750.789106	39.618023
2924.167595	286153.203864	39.623040
2926.870128	286571.621387	39.628058
2930.072257	286970.221206	39.633076
2932.871295	287381.636676	39.638093
2935.549758	287798.608573	39.643111
2938.978239	288200.905337	39.648128
2941.728121	288615.705623	39.653146
2944.539168	289031.867417	39.658164
2947.576416	289456.121711	39.663181
2950.298227	289871.153314	39.668199
2953.620234	290267.519898	39.673216
2956.338702	290682.804840	39.678234
2959.162965	291069.418206	39.683252
2962.282856	291446.661439	39.688269
2964.874303	291819.796344	39.693287
2967.689122	292194.698904	39.698304
2970.465956	292587.160014	39.703322
2973.283660	292966.023695	39.708340
2976.062490	293358.152962	39.713357
2978.878936	293762.290908	39.718375
2981.882994	294144.120593	39.723392
2984.730063	294558.438547	39.728410
2987.786629	294966.168758	39.733428
2990.729806	295372.900032	39.738445
2993.649418	295790.379314	39.743463
2996.576342	296208.161389	39.748480
2999.163984	296628.231652	39.753498
3002.131376	297056.318698	39.758516
3005.058410	297491.777702	39.763533
3008.320314	297931.246958	39.768551
3011.453653	298358.237831	39.773568
3014.505233	298808.965797	39.778586
3017.494551	299250.126036	39.783604
3020.686821	299692.192866	39.788621
3023.535258	300140.866537	39.793639
3026.755061	300583.434663	39.798656
3029.741674	301029.137451	39.803674
3033.152586	301476.930937	39.808692
3036.203164	301931.232077	39.813709
3038.800865	302381.183754	39.818727
3042.321069	302825.450646	39.823744
3045.244717	303295.668821	39.828762
3048.519620	303748.354070	39.833780
3051.754616	304190.807680	39.838797
3054.827755	304649.846799	39.843815
3057.929977	305105.679318	39.848832
3061.151894	305569.568754	39.853850
3063.967892	306027.424724	39.858868
3067.088687	306480.531805	39.863885
3069.916696	306947.349014	39.868903
3073.622918	307408.843900	39.873920
3076.430238	307877.769207	39.878938
3079.473677	308345.740988	39.883956
3082.608737	308796.627751	39.888973
3085.594920	309261.303110	39.893991
3089.092527	309732.372664	39.899008
3092.092866	310199.658299	39.904026
3095.408179	310653.151080	39.909044
3098.398881	311111.443143	39.914061
3101.379800	311578.396076	39.919079
3104.690562	312039.783243	39.924096
3107.911962	312511.291477	39.929114
3111.263619	312969.290206	39.934132
3114.499510	313434.772590	39.939149
3117.292843	313893.058934	39.944167
3120.543951	314349.518341	39.949184
3123.453726	314799.019768	39.954202
3126.586408	315239.492916	39.959220
3129.614713	315660.754142	39.964237
3132.466132	316084.225850	39.969255
3135.566345	316495.211315	39.974272
3138.522109	316932.631870	39.979290
3141.318402	317367.180345	39.984308
3144.504952	317793.817204	39.989325
3147.378849	318242.699205	39.994343
3150.361026	318682.545820	39.999360
3153.439796	319140.483461	40.004378
3156.515454	319586.939759	40.009396
3159.694354	320035.155359	40.014413
3162.506473	320510.423856	40.019431
3165.825616	320982.866755	40.024448
3168.790402	321454.118783	40.029466
3171.909337	321928.416900	40.034484
3175.385293	322408.928890	40.039501
3178.157035	322891.962292	40.044519
3181.652617	323376.249838	40.049536
3184.841807	323866.297212	40.054554
3188.253806	324355.163657	40.059572
3191.440599	324845.332648	40.064589
3194.520824	325346.511880	40.069607
3197.790887	325826.833720	40.074624
3201.039237	326321.986995	40.079642
3204.426439	326834.028399	40.084660
3207.996902	327333.340007	40.089677
3211.293468	327824.235292	40.094695
3214.326836	328319.968705	40.099712
3217.516873	328819.407126	40.104730
3220.827117	329327.609690	40.109748
3224.213254	329825.131282	40.114765
3227.616829	330334.023309	40.119783
3230.880316	330827.494568	40.124800
3234.307522	331345.416072	40.129818
3237.538587	331841.831273	40.134836
3240.645458	332346.413945	40.139853
3243.631142	332848.320558	40.144871
3247.305666	333368.016646	40.149888
3250.648379	333875.293551	40.154906
3253.910928	334379.253018	40.159924
3257.465822	334896.112656	40.164941
3260.480227	335402.820850	40.169959
3264.212917	335908.573698	40.174976
3267.494571	336412.997543	40.179994
3270.154424	336915.510001	40.185012
3274.008898	337424.253690	40.190029
3277.246131	337937.356793	40.195047
3280.917894	338431.953253	40.200064
3284.014546	338949.260098	40.205082
3287.410245	339456.841646	40.210100
3290.824079	339952.152711	40.215117
3293.908994	340465.640507	40.220135
3296.843424	340961.121006	40.225152
3300.295506	341456.007874	40.230170
3303.234204	341923.271937	40.235188
3306.695389	342396.467073	40.240205
3309.889532	342863.734302	40.245223
3312.912159	343325.998018	40.250240
3315.856566	343793.221355	40.255258
3319.021125	344281.174073	40.260276
3322.373944	344754.672381	40.265293
3325.225699	345237.639747	40.270311
3328.353437	345730.866971	40.275328
3331.656798	346233.201800	40.280346
3334.312391	346739.874405	40.285364
3337.632405	347243.594046	40.290381
3340.657268	347770.686595	40.295399
3344.037916	348292.082059	40.300416
3347.259728	348833.807033	40.305434
3350.439242	349370.024569	40.310452
3353.960368	349918.926658	40.315469
3357.389301	350472.610342	40.320487
3361.008251	351016.814892	40.325504
3364.464249	351568.731453	40.330522
3367.731440	352123.540679	40.335540
3371.159450	352675.424805	40.340557
3374.648295	353233.284265	40.345575
3378.084445	353788.201535	40.350592
3381.704307	354348.262145	40.355610
3384.928686	354913.963618	40.360628
3388.553822	355470.102072	40.365645
3392.220482	356037.624888	40.370663
3395.609565	356596.098164	40.375680
3399.339550	357160.983854	40.380698
3402.643105	357730.575515	40.385716
3406.225916	358286.892450	40.390733
3409.527941	358858.451100	40.395751
3413.365467	359426.923366	40.400768
3417.011651	359998.287274	40.405786
3420.240646	360560.268716	40.410804
3423.970410	361112.139074	40.415821
3427.168557	361685.939406	40.420839
3430.835630	362253.288259	40.425856
3434.372501	362811.920260	40.430874
3438.044362	363386.157824	40.435892
3441.348128	363940.016418	40.440909
3444.684557	364511.146013	40.445927
3447.975130	365070.804718	40.450944
3451.606999	365647.152025	40.455962
3454.981416	366208.915134	40.460980
3458.729464	366774.241079	40.465997
3462.441612	367341.950959	40.471015
3465.880318	367918.020342	40.476032
3469.288888	368484.570804	40.481050
3472.996404	369054.111776	40.486068
3476.553125	369604.586590	40.491085
3480.204883	370166.509029	40.496103
3483.795920	370726.911206	40.501120
3486.994765	371262.035426	40.506125
3489.595736	371778.630650	40.511130
3493.675305	372219.126613	40.516135
3496.802591	372624.993685	40.521140
3499.152255	372974.836837	40.526144
3501.881660	373277.047231	40.531149
3504.218833	373528.695356	40.536154
3505.971923	373725.386224	40.541159
3507.522759	373898.832351	40.546164
3509.107696	374018.115006	40.551168
3510.576153	374103.964916	40.556173
3511.424772	374161.218746	40.561178
3512.805331	374187.990192	40.566183
3513.753110	374183.287127	40.571188
3514.449134	374164.098849	40.576192
3515.036866	374099.673693	40.581197
3515.168264	374053.941144	40.586202
3515.600042	373965.425276	40.591207
3515.907665	373886.595297	40.596212
3516.018927	373781.213415	40.601216
3516.409575	373662.966264	40.606221
3516.275123	373556.630567	40.611226
3516.244354	373407.948864	40.616231
3515.846628	373283.134988	40.621236
3515.995268	373147.601077	40.626240
3515.933495	373018.154367	40.631245
3515.762787	372868.399000	40.636250
3516.062332	372717.322255	40.641255
3515.770440	372582.212295	40.646260
3515.513254	372429.823392	40.651264
3515.353171	372274.060635	40.656269
3514.660649	372131.253660	40.661274
3514.841168	371978.310577	40.666279
3514.443047	371828.256741	40.671284
3513.930615	371696.307830	40.676288
3513.898271	371559.474554	40.681293
3513.476446	371418.861042	40.686298
3513.623915	371287.620595	40.691303
3513.068836	371165.445580	40.696308
3512.641556	371016.080345	40.701312
3512.990649	370895.211674	40.706317
3512.248569	370773.930053	40.711322
3512.245840	370640.141923	40.716327
3512.114065	370536.698331	40.721332
3511.790848	370409.981604	40.726336
3511.508672	370304.933061	40.731341
3511.301706	370190.586677	40.736346
3511.235420	370086.902683	40.741351
3511.026154	369970.368209	40.746356
3510.242834	369870.613112	40.751360
3510.235288	369767.453311	40.756365
3509.768080	369674.822007	40.761370
3509.892224	369582.071573	40.766375
3509.761945	369491.498180	40.771380
3509.532925	369406.791574	40.776384
3509.268757	369317.968955	40.781389
3509.061740	369239.644177	40.786394
3508.956218	369145.606195	40.791399
3508.723671	369078.224736	40.796404
3508.702702	368996.664551	40.801408
3508.454646	368914.326002	40.806413
3508.160528	368855.756522	40.811418
3508.276063	368777.939620	40.816423
3507.897786	368713.862538	40.821428
3507.566256	368645.783707	40.826432
3507.560691	368591.951191	40.831437
3507.540617	368528.580441	40.836442
3507.497128	368467.274044	40.841447
3507.576086	368405.159522	40.846452
3507.419543	368358.168858	40.851456
3507.458603	368295.984165	40.856461
3507.016330	368243.136152	40.861466
3506.947174	368184.784619	40.866471
3506.995551	368126.134571	40.871476
3506.771957	368088.694769	40.876480
3507.107034	368035.062129	40.881485
3506.625492	367983.085022	40.886490
3506.687804	367935.474149	40.891495
3506.701733	367889.931643	40.896500
3506.495527	367845.059934	40.901504
3506.624367	367800.669484	40.906509
3506.130036	367752.942884	40.911514
3506.035103	367710.953799	40.916519
3506.194370	367672.155584	40.921524
3506.169751	367632.063436	40.926528
3506.134078	367592.329185	40.931533
3505.910138	367560.460736	40.936538
3506.126787	367514.784026	40.941543
3505.822142	367470.283684	40.946548
3505.554160	367438.320343	40.951552
3505.711800	367404.508756	40.956557
3505.702165	367378.279835	40.961562
3505.726082	367344.082273	40.966567
3505.604462	367311.637746	40.971572
3505.316874	367282.272469	40.976576
3505.498235	367250.975768	40.981581
3505.492100	367218.182169	40.986586
3505.486064	367188.390687	40.991591
3505.462448	367156.235856	40.996596
3505.404590	367121.745746	41.001600
3505.651299	367096.086739	41.006605
3505.407580	367059.514275	41.011610
3505.110772	367030.252057	41.016615
3505.006725	367001.442745	41.021620
3505.126458	366971.478581	41.026624
3505.319779	366958.625327	41.031629
3504.905725	366934.902527	41.036634
3505.045675	366908.980426	41.041639
3504.914693	366883.788084	41.046644
3504.650052	366858.744070	41.051648
3504.633910	366843.634101	41.056653
3504.863212	366834.260704	41.061658
3504.994185	366803.658595	41.066663
3505.016204	366778.009486	41.071668
3504.713559	366753.811015	41.076672
3504.540091	366724.274673	41.081677
3504.407168	366715.263826	41.086682
3504.967557	366687.774032	41.091687
3504.623159	366667.576556	41.096692
3504.371750	366657.159661	41.101696
3504.663461	366626.353921	41.106701
3504.925821	366616.695387	41.111706
3504.643491	366593.867503	41.116711
3504.627262	366579.520729	41.121716
3504.498958	366554.683970	41.126720
3504.477159	366539.320368	41.131725
3503.941895	366530.932826	41.136730
3504.339315	366520.260666	41.141735
3504.822214	366505.529647	41.146740
3504.308487	366491.617691	41.151744
3504.533444	366468.022597	41.156749
3504.542449	366450.745913	41.161754
3504.413173	366441.251028	41.166759
3504.147219	366416.308743	41.171764
3504.425123	366403.899921	41.176768
3504.457089	366379.572018	41.181773
3504.305600	366377.255407	41.186778
3504.668643	366350.585323	41.191783
3504.662783	366336.287716	41.196788
3504.325234	366326.520425	41.201792
3504.357043	366300.538741	41.206797
3504.582894	366291.979937	41.211802
3504.820204	366267.950261	41.216807
3504.342153	366252.938562	41.221812
3504.173832	366234.519473	41.226816
3504.551747	366214.945428	41.231821
3504.125934	366204.632328	41.236826
3504.029381	366184.013811	41.241831
3503.920048	366177.085418	41.246836
3503.943846	366163.241033	41.251840
3504.066796	366152.357752	41.256845
3503.885348	366138.698465	41.261850
3504.050415	366123.890357	41.266855
3503.941929	366120.091263	41.271860
3504.073548	366106.789552	41.276864
3504.299100	366098.052661	41.281869
3504.059516	366094.935799	41.286874
3504.515692	366084.127033	41.291879
3504.164072	366064.159409	41.296884
3504.238984	366047.889856	41.301888
3504.049297	366039.778340	41.306893
3503.807535	366027.985869	41.311898
3504.096433	366002.701205	41.316903
3504.082499	366011.354067	41.321908
3504.046826	365991.794428	41.326912
3504.125772	365980.129340	41.331917
3504.214546	365969.963814	41.336922
3503.860685	365960.326235	41.341927
3504.454194	365946.951452	41.346932
3504.307435	365933.057633	41.351936
3504.483373	365909.342782	41.356941
3504.098537	365913.856250	41.361946
3504.228662	365891.471654	41.366951
3504.156647	365881.585957	41.371956
3504.049264	365874.224682	41.376960
3504.077755	365846.335052	41.381965
3503.955382	365837.729445	41.386970
3504.254452	365823.510680	41.391975
3504.122860	365806.179647	41.396980
3504.073520	365806.696451	41.401984
3503.977107	365782.083207	41.406989
3503.995375	365780.401241	41.411994
3504.067609	365752.428309	41.416999
3504.110643	365747.892829	41.422004
3504.079856	365735.430856	41.427008
3504.108633	365712.782323	41.432013
3504.184748	365709.819065	41.437018
3504.209302	365694.829489	41.442023
3504.014101	365693.181268	41.447028
3504.042214	365681.625910	41.452032
3504.004500	365663.898338	41.457037
3503.630010	365652.737382	41.462042
3503.768509	365644.141380	41.467047
3503.732691	365632.367131	41.472052
3504.030505	365627.613258	41.477056
3504.288301	365615.410941	41.482061
3503.787812	365604.142678	41.487066
3503.633627	365590.784229	41.492071
3503.560851	365585.834513	41.497076
3503.655252	365569.663477	41.502080
3503.982469	365572.054413	41.507085
3503.745070	365559.955814	41.512090
3504.008788	365548.235958	41.517095
3504.122219	365539.796557	41.522100
3503.844151	365523.124647	41.527104
3503.972789	365509.925003	41.532109
3503.946924	365503.873814	41.537114
3503.759928	365488.535970	41.542119
3504.019827	365480.709476	41.547124
3503.911881	365467.267351	41.552128
3503.859517	365464.171732	41.557133
3503.505694	365451.328221	41.562138
3504.087934	365440.524813	41.567143
3504.033204	365432.188307	41.572148
3503.747019	365414.576249	41.577152
3503.990511	365408.914993	41.582157
3504.098471	365391.113397	41.587162
3504.061126	365384.173500	41.592167
3504.089369	365361.702977	41.597172
3503.943071	365357.197391	41.602176
3503.945459	365338.598287	41.607181
3503.539208	365333.955697	41.612186
3503.967680	365320.988467	41.617191
3504.010620	365307.140794	41.622196
3503.728003	365305.557265	41.627200
3504.091035	365285.832513	41.632205
3504.310350	365278.979238	41.637210
3504.025667	365263.504103	41.642215
3503.513847	365257.427938	41.647220
3503.619928	365256.342703	41.652224
3503.722232	365235.132563	41.657229
3503.372328	365235.264360	41.662234
3503.515997	365227.659743	41.667239
3503.682160	365218.753969	41.672244
3503.673173	365204.151179	41.677248
3503.710623	365201.143115	41.682253
3503.807651	365208.099341	41.687258
3503.869557	365190.101402	41.692263
3503.639333	365183.522730	41.697268
3503.462658	365182.176879	41.702272
3503.700801	365157.510402	41.707277
3503.414160	365169.590481	41.712282
3503.400681	365163.053868	41.717287
3503.773955	365159.331185	41.722292
3503.423130	365140.686071	41.727296
3503.410511	365143.563291	41.732301
3503.278875	365139.538786	41.737306
3503.511654	365141.283152	41.742311
3503.627911	365136.125398	41.747316
3503.652974	365122.255051	41.752320
3503.777761	365118.673424	41.757325
3503.611175	365108.344531	41.762330
3503.688206	365093.906209	41.767335
3503.950294	365096.002148	41.772340
3503.703161	365077.849478	41.777344
3503.662673	365064.956319	41.782349
3503.617077	365074.301333	41.787354
3503.706481	365047.419309	41.792359
3503.743821	365043.317194	41.797364
3503.736742	365040.952240	41.802368
3503.865678	365014.063946	41.807373
3503.635792	365020.842897	41.812378
3503.664304	365014.986591	41.817383
3503.591041	364993.753209	41.822388
3503.492879	364995.117368	41.827392
3503.656905	364990.079262	41.832397
3503.678552	364982.646555	41.837402
3503.899072	364963.249513	41.842407
3503.612085	364963.244146	41.847412
3503.748999	364943.809427	41.852416
3504.170226	364937.407601	41.857421
3504.044930	364930.710530	41.862426
3503.843670	364906.724025	41.867431
3503.982495	364907.719956	41.872436
3503.723002	364885.600007	41.877440
3503.882955	364874.125373	41.882445
3503.698891	364866.954160	41.887450
3503.685298	364854.285679	41.892455
3503.918840	364847.938956	41.897460
3503.724158	364851.811826	41.902464
3504.333304	364827.977031	41.907469
3504.039704	364814.665838	41.912474
3504.020345	364794.975885	41.917479
3503.942982	364788.780082	41.922484
3503.615331	364772.217508	41.927488
3503.979294	364755.494697	41.932493
3503.182778	364753.992397	41.937498
3503.060221	364743.147592	41.942503
3503.301677	364732.372452	41.947508
3503.389655	364732.867557	41.952512
3503.625426	364740.794213	41.957517
3503.696516	364734.727592	41.962522
3503.757753	364711.437342	41.967527
3503.437333	364707.875183	41.972532
3503.712504	364709.689194	41.977536
3503.600465	364701.819596	41.982541
3503.309236	364693.113251	41.987546
3503.620639	364689.832850	41.992551
3503.362656	364691.273173	41.997556
3503.347811	364679.240926	42.002560
3503.747951	364658.136090	42.007565
3503.411662	364664.117726	42.012570
3503.376355	364661.655441	42.017575
3503.360677	364658.452194	42.022580
3503.397192	364641.730224	42.027584
3503.628574	364643.067736	42.032589
3503.152284	364649.987472	42.037594
3503.459827	364651.923585	42.042599
3503.514452	364621.001300	42.047604
3503.665445	364630.035447	42.052608
3503.886448	364621.884190	42.057613
3503.485171	364606.554482	42.062618
3503.897805	364594.887168	42.067623
3503.891251	364591.097273	42.072628
3503.552877	364572.500843	42.077632
3503.743992	364560.461447	42.082637
3503.586999	364557.662186	42.087642
3503.884978	364550.134834	42.092647
3504.067572	364529.573203	42.097652
3503.562089	364530.289355	42.102656
3503.774803	364499.392880	42.107661
3503.148941	364509.771161	42.112666
3503.490121	364503.610922	42.117671
3503.573087	364501.613356	42.122676
3503.450330	364487.918848	42.127680
3503.374740	364485.971793	42.132685
3503.215884	364491.670964	42.137690
3503.638543	364481.833970	42.142695
3503.573906	364465.814904	42.147700
3503.481577	364454.558155	42.152704
3503.489551	364453.971839	42.157709
3503.716405	364447.040917	42.162714
3503.740619	364444.543767	42.167719
3504.038195	364437.627105	42.172724
3504.092402	364421.207581	42.177728
3504.176735	364396.336017	42.182733
3503.654042	364399.802799	42.187738
3503.572132	364368.978260	42.192743
3503.705285	364369.110017	42.197748
3503.450712	364365.384759	42.202752
3503.672831	364345.452886	42.207757
3503.630972	364342.202868	42.212762
3503.455967	364342.739556	42.217767
3503.470816	364322.280683	42.222772
3503.487761	364316.298898	42.227776
3503.533443	364311.533864	42.232781
3503.566220	364321.909830	42.237786
3503.487524	364296.300678	42.242791
3503.836667	364274.923848	42.247796
3503.400679	364286.340793	42.252800
3504.081594	364271.017984	42.257805
3503.488088	364264.522056	42.262810
3503.383502	364245.990306	42.267815
3503.352713	364259.378690	42.272820
3503.511049	364245.308900	42.277824
3503.664574	364220.248196	42.282829
3503.370806	364227.368131	42.287834
3503.746476	364226.316581	42.292839
3503.812199	364210.098710	42.297844
3503.579208	364198.889580	42.302848
3503.818492	364195.188004	42.307853
3503.744555	364181.282135	42.312858
3503.680966	364173.760998	42.317863
3503.529383	364176.634806	42.322868
3503.220761	364148.263114	42.327872
3503.445640	364137.388680	42.332877
3503.352271	364141.576360	42.337882
3503.782515	364135.376546	42.342887
3503.964844	364114.585777	42.347892
3503.531523	364116.918926	42.352896
3503.567357	364111.315784	42.357901
3503.265262	364093.858392	42.362906
3503.268616	364086.402988	42.367911
3503.384582	364085.468825	42.372916
3503.594408	364089.837569	42.377920
3504.027636	364065.877528	42.382925
3503.317746	364057.949677	42.387930
3503.061427	364056.870822	42.392935
3503.417783	364062.386816	42.397940
3503.230697	364054.121871	42.402944
3503.149769	364051.437772	42.407949
3503.132527	364036.734139	42.412954
3503.452093	364029.279620	42.417959
3503.475540	364029.835823	42.422964
3503.327138	364037.976001	42.427968
3503.676014	364027.718032	42.432973
3503.375830	364019.343742	42.437978
3503.446526	364003.786550	42.442983
3503.423301	364015.799843	42.447988
3503.199200	364010.034235	42.452992
3503.170445	363994.492762	42.457997
3503.539214	363989.396732	42.463002
3503.606560	363991.523512	42.468007
3503.838548	364000.137877	42.473012
3503.512880	363986.246304	42.478016
3503.655856	363957.624990	42.483021
3503.555080	363970.515646	42.488026
3503.189834	363973.092477	42.493031
3503.464926	363954.220700	42.498036
3503.625092	363934.858208	42.503040
3503.597421	363935.956815	42.508045
3503.816647	363938.059586	42.513050
3503.788572	363914.554056	42.518055
3503.619067	363905.497545	42.523060
3503.573956	363911.585906	42.528064
3503.725044	363887.695823	42.533069
3503.504191	363887.094790	42.538074
3503.527261	363889.483014	42.543079
3503.542908	363855.207784	42.548084
3503.287892	363853.416289	42.553088
3503.625333	363845.984358	42.558093
3503.140455	363855.831619	42.563098
3503.378121	363835.668072	42.568103
3503.373202	363825.618656	42.573108
3503.192564	363810.737232	42.578112
3503.386504	363813.327440	42.583117
3503.124161	363817.592752	42.588122
3503.452980	363807.465124	42.593127
3503.052310	363791.219066	42.598132
3503.282157	363787.315398	42.603136
3503.316023	363773.977572	42.608141
3503.045035	363785.037784	42.613146
3503.319645	363785.808721	42.618151
3503.569131	363784.929774	42.623156
3503.152470	363787.870959	42.628160
3503.377363	363763.104049	42.633165
3503.619625	363762.455240	42.638170
3503.382744	363759.032463	42.643175
3503.630245	363761.792313	42.648180
3503.487523	363746.828542	42.653184
3503.175233	363730.950149	42.658189
3503.268165	363735.286520	42.663194
3503.346387	363730.389060	42.668199
3503.662051	363715.607248	42.673204
3503.296522	363715.461634	42.678208
3503.390571	363699.824315	42.683213
3503.355658	363706.852518	42.688218
3503.513909	363709.931809	42.693223
3503.378502	363690.819497	42.698228
3503.021314	363673.625095	42.703232
3503.328057	363675.510489	42.708237
3502.855985	363681.717272	42.713242
3503.516471	363683.470406	42.718247
3503.630692	363676.353623	42.723252
3503.054664	363678.683911	42.728256
3503.088328	363659.977404	42.733261
3503.281933	363657.402542	42.738266
3502.941761	363667.379628	42.743271
3503.202620	363665.659230	42.748276
3503.336618	363666.401512	42.753280
3503.848047	363669.577632	42.758285
3503.189581	363651.820199	42.763290
3503.155083	363639.307351	42.768295
3503.076651	363634.103876	42.773300
3503.009369	363634.699873	42.778304
3503.116919	363638.321510	42.783309
3502.997296	363652.029443	42.788314
3502.969092	363647.632237	42.793319
3502.870121	363645.179963	42.798324
3503.047836	363647.136646	42.803329
3503.136127	363639.591409	42.808333
3503.073256	363659.982140	42.813338
3503.322468	363640.605446	42.818343
3503.621540	363628.268854	42.823348
3503.199863	363629.353429	42.828353
3503.558598	363623.699177	42.833357
3503.427103	363621.353820	42.838362
3503.262924	363606.749612	42.843367
3503.272438	363601.939334	42.848372
3503.297712	363594.683937	42.853377
3503.598900	363598.682067	42.858381
3503.208185	363607.700284	42.863386
3503.361179	363587.855343	42.868391
3503.223518	363578.462961	42.873396
3503.312708	363582.163837	42.878401
3503.464302	363573.896148	42.883405
3503.557922	363588.537260	42.888410
3503.365504	363564.395989	42.893415
3503.600330	363557.361896	42.898420
3503.350134	363548.267184	42.903425
3503.428599	363547.415272	42.908429
3503.266958	363542.835600	42.913434
3503.176043	363520.612008	42.918439
3503.578360	363522.049748	42.923444
3503.140905	363523.085932	42.928449
3503.697053	363518.392775	42.933453
3503.559386	363501.443487	42.938458
3503.316219	363499.980878	42.943463
3503.400307	363479.892345	42.948468
3503.108259	363491.973720	42.953473
3503.413315	363486.327938	42.958477
3503.388941	363478.647823	42.963482
3503.374168	363477.225436	42.968487
3503.336080	363458.173973	42.973492
3503.025074	363473.133535	42.978497
3503.285599	363463.092961	42.983501
3503.336205	363461.583905	42.988506
3503.487488	363435.505364	42.993511
3503.648679	363439.805527	42.998516
3503.399114	363450.557102	43.003521
3503.590225	363433.479477	43.008525
3503.352491	363425.044317	43.013530
3503.141929	363406.961534	43.018535
3503.407322	363409.718577	43.023540
3503.119543	363420.374425	43.028545
3503.321375	363408.485697	43.033549
3502.958055	363403.734344	43.038554
3503.220361	363385.322350	43.043559
3503.298038	363388.185405	43.048564
3503.047484	363383.416221	43.053569
3503.362201	363387.717561	43.058573
3503.371878	363386.443971	43.063578
3503.286979	363391.037486	43.068583
3503.362811	363368.329463	43.073588
3503.396514	363357.128852	43.078593
3503.463192	363367.830448	43.083597
3503.113339	363368.522011	43.088602
3503.621088	363357.729892	43.093607
3503.468878	363359.662415	43.098612
3503.214723	363344.588911	43.103617
3503.457628	363339.181935	43.108621
3503.439121	363341.525871	43.113626
3503.197686	363328.613105	43.118631
3503.242049	363318.912006	43.123636
3503.305471	363311.854087	43.128641
3503.496784	363302.664079	43.133645
3503.194436	363311.439384	43.138650
3503.065154	363312.045187	43.143655
3503.453457	363318.955650	43.148660
3503.027361	363296.479612	43.153665
3503.395673	363278.203481	43.158669
3503.120583	363287.915917	43.163674
3503.126988	363285.294299	43.168679
3503.253977	363283.416942	43.173684
3503.338555	363284.650484	43.178689
3503.165222	363281.395733	43.183693
3503.078311	363268.865626	43.188698
3503.228640	363266.297585	43.193703
3503.211739	363258.641696	43.198708
3503.005056	363263.050925	43.203713
3503.368777	363266.861088	43.208717
3503.331096	363271.777925	43.213722
3503.195262	363260.247875	43.218727
3503.290876	363235.933674	43.223732
3503.215090	363227.981759	43.228737
3503.564786	363219.631798	43.233741
3503.438662	363229.320694	43.238746
3503.377270	363230.450094	43.243751
3503.615606	363195.401284	43.248756
3503.260761	363204.286687	43.253761
3503.532689	363199.663877	43.258765
3503.403832	363201.516383	43.263770
3502.942827	363199.782874	43.268775
3503.396941	363175.691848	43.273780
3503.407493	363164.265852	43.278785
3503.290806	363174.156822	43.283789
3503.381153	363184.931052	43.288794
3503.801307	363184.559441	43.293799
3503.733353	363160.958056	43.298804
3503.389021	363159.587763	43.303809
3503.480063	363154.179330	43.308813
3503.352267	363151.273591	43.313818
3503.371214	363124.605135	43.318823
3503.455341	363106.348422	43.323828
3503.329660	363122.932675	43.328833
3503.651004	363112.780633	43.333837
3503.073468	363106.053018	43.338842
3503.379681	363090.458283	43.343847
3503.539276	363080.153696	43.348852
3503.000750	363093.749913	43.353857
3503.191994	363101.683891	43.358861
3503.150352	363115.125212	43.363866
3503.322540	363092.045599	43.368871
3502.981026	363056.146920	43.373876
3502.784796	363071.826349	43.378881
3502.939644	363059.257964	43.383885
3502.789394	363067.678493	43.388890
3502.973231	363061.619270	43.393895
3503.438119	363062.182027	43.398900
3503.128763	363062.663637	43.403905
3503.558985	363065.318308	43.408909
3503.157314	363069.503939	43.413914
3503.203912	363064.611410	43.418919
3503.301056	363051.848591	43.423924
3503.138618	363049.737096	43.428929
3503.441299	363031.929243	43.433933
3503.365004	363042.399075	43.438938
3503.295738	363040.959846	43.443943
3503.407201	363021.630116	43.448948
3503.000450	363020.905796	43.453953
3503.671877	363013.013820	43.458957
3503.251918	363010.866704	43.463962
3503.250229	363009.162346	43.468967
3503.430831	363004.223180	43.473972
3503.160316	362991.874693	43.478977
3503.596731	362985.775528	43.483981
3503.183639	362987.723869	43.488986
3503.112339	362981.170642	43.493991
3503.409858	362974.966213	43.498996
3503.317876	362958.772836	43.504001
3503.451170	362957.428801	43.509005
3503.260006	362952.192184	43.514010
3503.307169	362950.225657	43.519015
3503.781565	362950.252579	43.524020
3503.384942	362931.028585	43.529025
3503.494162	362919.510596	43.534029
3503.206065	362924.975949	43.539034
3503.122565	362926.821294	43.544039
3503.491693	362922.437534	43.549044
3503.179505	362898.213074	43.554049
3503.323045	362895.213531	43.559053
3503.253191	362888.990840	43.564058
3503.420523	362890.287642	43.569063
3503.464502	362883.690731	43.574068
3503.196358	362872.792169	43.579073
3503.344423	362867.349244	43.584077
3503.437564	362864.434000	43.589082
3503.215427	362870.194264	43.594087
3503.268453	362856.191590	43.599092
3503.119108	362872.067230	43.604097
3503.160071	362843.563133	43.609101
3503.048005	362837.626998	43.614106
3503.331092	362840.050500	43.619111
3503.151228	362837.865417	43.624116
3502.892413	362839.942038	43.629121
3503.185561	362835.315838	43.634125
3503.041036	362838.214057	43.639130
3503.063251	362844.419137	43.644135
3503.202259	362833.786972	43.649140
3503.016208	362836.564535	43.654145
3502.971254	362813.417336	43.659149
3502.976140	362820.032270	43.664154
3503.044301	362810.836191	43.669159
3503.293413	362816.827291	43.674164
3503.209495	362830.020933	43.679169
3503.518899	362815.265268	43.684173
3503.393284	362823.554723	43.689178
3502.901238	362802.030316	43.694183
3503.068035	362795.312198	43.699188
3503.153403	362784.001502	43.704193
3503.608760	362788.916774	43.709197
3503.025497	362790.866582	43.714202
3503.219442	362795.339738	43.719207
3503.536924	362793.559467	43.724212
3503.347563	362776.134642	43.729217
3503.331443	362766.035878	43.734221
3503.147100	362758.660824	43.739226
3503.317592	362757.692570	43.744231
3503.588500	362750.830762	43.749236
3503.563763	362745.593254	43.754241
3503.482958	362730.746588	43.759245
3503.478067	362724.437271	43.764250
3503.526666	362732.902755	43.769255
3503.474105	362715.608946	43.774260
3502.853362	362708.786325	43.779265
3503.386747	362710.839483	43.784269
3503.199190	362706.441937	43.789274
3503.287250	362704.290822	43.794279
3503.107361	362714.751662	43.799284
3503.046214	362705.423339	43.804289
3503.168503	362701.841919	43.809293
3503.058520	362687.076186	43.814298
3503.041042	362670.209371	43.819303
3503.326587	362659.452221	43.824308
3503.241867	362673.231259	43.829313
3502.981475	362674.544801	43.834317
3502.938148	362682.973938	43.839322
3503.086890	362678.395998	43.844327
3503.248789	362669.643073	43.849332
3502.938779	362682.465389	43.854337
3503.441728	362663.811508	43.859341
3502.806551	362660.578843	43.864346
3502.849490	362641.056232	43.869351
3503.127492	362639.205864	43.874356
3503.327538	362647.672864	43.879361
3503.413485	362648.091980	43.884365
3503.440908	362648.927462	43.889370
3503.294120	362643.276681	43.894375
3503.360006	362630.595023	43.899380
3503.161338	362616.555736	43.904385
3503.461709	362620.528635	43.909389
3503.345397	362626.068642	43.914394
3503.230594	362624.280375	43.919399
3503.479589	362607.753077	43.924404
3503.178611	362601.846778	43.929409
3502.794695	362593.002021	43.934413
3503.042428	362587.212526	43.939418
3503.322500	362595.463326	43.944423
3503.234387	362600.515431	43.949428
3503.044565	362607.746403	43.954433
3503.590576	362596.973504	43.959437
3503.151656	362578.799279	43.964442
3503.196839	362576.680382	43.969447
3503.053034	362567.772213	43.974452
3503.050989	362561.564202	43.979457
3503.120588	362565.319146	43.984461
3503.120576	362569.899322	43.989466
3503.261729	362556.645962	43.994471
3503.320817	362567.501610	43.999476
3502.924964	362556.572276	44.004481
3503.168892	362543.938780	44.009485
3502.772193	362543.747199	44.014490
3502.655735	362543.205977	44.019495
3503.173540	362542.386365	44.024500
3503.090051	362547.997525	44.029505
3502.935369	362546.113782	44.034509
3503.014532	362559.332607	44.039514
3503.159650	362553.941000	44.044519
3503.144089	362556.233621	44.049524
3502.766981	362555.988054	44.054529
3503.236992	362548.153288	44.059533
3502.733987	362558.996028	44.064538
3502.634227	362549.546555	44.069543
3503.337416	362565.389291	44.074548
3503.242217	362564.157704	44.079553
3502.995946	362539.032075	44.084557
3503.334841	362541.370436	44.089562
3503.073942	362532.735219	44.094567
3503.218683	362534.849830	44.099572
3502.952247	362542.169259	44.104577
3503.271557	362529.422062	44.109581
3503.220661	362537.343530	44.114586
3503.025329	362539.053904	44.119591
3503.152440	362533.207139	44.124596
3503.063431	362529.531889	44.129601
3503.195091	362511.750876	44.134605
3503.098023	362519.654203	44.139610
3503.032750	362512.794622	44.144615
3503.343505	362502.924013	44.149620
3503.335321	362518.624787	44.154625
3503.380201	362508.770769	44.159629
3503.042378	362496.280124	44.164634
3503.161478	362488.704385	44.169639
3503.641373	362475.982674	44.174644
3503.327537	362482.622601	44.179649
3503.462929	362469.904466	44.184653
3503.112139	362468.865953	44.189658
3503.055268	362442.972433	44.194663
3503.103452	362440.089715	44.199668
3503.221033	362449.943801	44.204673
3503.373770	362453.812833	44.209677
3503.586538	362455.611356	44.214682
3502.922733	362457.930137	44.219687
3503.548366	362445.032708	44.224692
3502.927593	362429.431642	44.229697
3503.430201	362423.271050	44.234701
3503.222457	362418.571332	44.239706
3503.163160	362411.481789	44.244711
3503.357311	362423.206681	44.249716
3502.977140	362425.709622	44.254721
3503.347847	362396.237111	44.259725
3502.850268	362393.186229	44.264730
3503.131503	362393.370915	44.269735
3502.668453	362391.586808	44.274740
3503.035304	362391.910626	44.279745
3503.037317	362389.009760	44.284749
3503.302365	362393.548047	44.289754
3503.285625	362392.583943	44.294759
3503.215654	362400.406671	44.299764
3503.092072	362399.942908	44.304769
3502.958536	362391.236640	44.309773
3503.184655	362378.478690	44.314778
3503.074255	362361.193895	44.319783
3503.285306	362360.550001	44.324788
3503.208865	362364.938723	44.329793
3503.452156	362361.465371	44.334797
3503.360524	362364.915040	44.339802
3503.538691	362346.643162	44.344807
3503.533822	362342.191254	44.349812
3503.163560	362341.028594	44.354817
3503.195431	362338.275672	44.359821
3503.194298	362338.250554	44.364826
3503.036674	362335.782039	44.369831
3503.338481	362307.948828	44.374836
3503.186586	362307.514984	44.379841
3503.264192	362305.441838	44.384845
3503.140237	362306.174035	44.389850
3502.962792	362311.672855	44.394855
3503.093537	362302.212334	44.399860
3502.850870	362303.777531	44.404865
3503.119983	362310.350762	44.409869
3503.143054	362315.258095	44.414874
3503.075522	362304.887468	44.419879
3502.874782	362300.924528	44.424884
3502.797979	362293.252506	44.429889
3503.025706	362290.036056	44.434893
3502.913940	362298.145302	44.439898
3502.705822	362292.122504	44.444903
3503.021637	362282.149270	44.449908
3502.781240	362302.339661	44.454913
3502.802875	362296.814879	44.459917
3503.224744	362301.404715	44.464922
3503.108273	362294.578641	44.469927
3503.202609	362294.894656	44.474932
3503.174085	362308.003353	44.479937
3503.720678	362294.456816	44.484941
3503.213081	362290.822282	44.489946
3503.253186	362280.638190	44.494951
3503.341991	362262.227739	44.499956
3502.795509	362279.056935	44.504961
3503.080976	362278.503054	44.509965
3503.177085	362277.393882	44.514970
3502.973279	362285.008786	44.519975
3503.100271	362282.495270	44.524980
3503.177106	362284.111734	44.529985
3503.172498	362266.657509	44.534989
3503.283855	362265.138810	44.539994
3503.184664	362252.305034	44.544999
3503.372413	362245.990641	44.550004
3503.037654	362250.292990	44.555009
3503.094055	362253.871932	44.560013
3503.077255	362257.411557	44.565018
3502.872716	362254.161668	44.570023
3503.311506	362245.721113	44.575028
3502.858354	362250.372962	44.580033
3503.119546	362234.276164	44.585037
3503.119650	362224.810838	44.590042
3503.036705	362220.142259	44.595047
3503.157309	362231.090038	44.600052
3502.901116	362237.390105	44.605057
3503.229177	362230.926302	44.610061
3503.355205	362239.328744	44.615066
3503.397891	362229.017008	44.620071
3503.250033	362224.358693	44.625076
3502.835529	362209.539174	44.630081
3503.126945	362207.533999	44.635085
3503.232295	362203.140987	44.640090
3502.906024	362210.342703	44.645095
3503.424380	362197.971064	44.650100
3502.915983	362214.463479	44.655105
3502.953585	362208.071039	44.660109
3503.169803	362222.922201	44.665114
3503.361811	362205.742206	44.670119
3503.317485	362183.536054	44.675124
3503.009623	362190.582194	44.680129
3503.136974	362178.068809	44.685133
3503.181661	362186.789459	44.690138
3503.209538	362181.263676	44.695143
3503.583766	362175.454132	44.700148
3503.056082	362168.845721	44.705153
3503.055674	362147.548622	44.710157
3503.093311	362154.972706	44.715162
3503.050420	362154.547072	44.720167
3503.204112	362148.772391	44.725172
3502.847960	362153.968700	44.730177
3503.260442	362144.412715	44.735181
3503.148941	362152.750947	44.740186
3503.007636	362148.880377	44.745191
3503.561665	362149.912504	44.750196
3503.582094	362137.390567	44.755201
3503.613310	362116.088454	44.760205
3503.182523	362121.525569	44.765210
3503.142945	362109.776458	44.770215
3503.318993	362097.866029	44.775220
3502.944696	362089.579441	44.780225
3503.136088	362080.898078	44.785229
3503.273922	362088.433556	44.790234
3503.072831	362081.849833	44.795239
3503.257398	362087.291444	44.800244
3503.346580	362086.590480	44.805249
3503.105401	362087.163100	44.810253
3503.141463	362059.778874	44.815258
3503.339761	362051.350862	44.820263
3503.335012	362043.565628	44.825268
3503.164385	362055.755402	44.830273
3503.260044	362049.022978	44.835277
3503.633818	362055.248915	44.840282
3503.170430	362037.587245	44.845287
3503.134551	362033.470994	44.850292
3503.140110	362022.045508	44.855297
3503.276181	362007.037099	44.860301
3503.247699	362021.341780	44.865306
3503.265216	362022.687737	44.870311
3503.585088	362007.828384	44.875316
3503.025974	362002.191825	44.880321
3503.216383	361982.391176	44.885325
3503.294466	361989.681667	44.890330
3502.939321	361985.157879	44.895335
3503.415644	361982.258334	44.900340
3502.974591	361990.012575	44.905345
3503.404072	361971.090140	44.910349
3503.251994	361959.587782	44.915354
3503.109604	361959.254212	44.920359
3503.286962	361945.358833	44.925364
3503.348612	361947.919171	44.930369
3503.130495	361960.828936	44.935373
3503.561099	361949.030893	44.940378
3502.999724	361937.364235	44.945383
3503.052922	361928.144904	44.950388
3502.858341	361932.501454	44.955393
3502.987429	361916.094649	44.960397
3503.193719	361929.598892	44.965402
3503.159150	361929.171940	44.970407
3503.264531	361922.208957	44.975412
3503.111261	361920.706640	44.980417
3503.148059	361918.054695	44.985421
3502.980570	361895.231755	44.990426
3502.939086	361893.304644	44.995431
3502.834766	361892.023591	45.000436
3502.740632	361899.264989	45.005441
3503.021504	361893.063050	45.010445
3503.083935	361901.373828	45.015450
3502.918059	361895.649640	45.020455
3503.193320	361895.428153	45.025460
3502.926162	361909.516153	45.030465
3502.810242	361908.160600	45.035469
3503.025782	361902.605115	45.040474
3503.068347	361906.975065	45.045479
3503.167473	361905.076613	45.050484
3503.054261	361912.855369	45.055489
3503.075749	361906.923446	45.060493
3502.925975	361908.321300	45.065498
3502.963855	361902.768458	45.070503
3503.307380	361873.503476	45.075508
3503.224091	361876.290293	45.080513
3503.009871	361877.622002	45.085517
3503.206315	361875.784499	45.090522
3502.751886	361885.525579	45.095527
3503.158234	361868.871362	45.100532
3503.016577	361890.751132	45.105537
3503.554553	361884.584879	45.110541
3503.238096	361878.808161	45.115546
3503.019535	361868.435870	45.120551
3503.404844	361840.792740	45.125556
3502.951852	361863.485095	45.130561
3503.226187	361853.950892	45.135565
3503.282968	361860.735872	45.140570
3503.128360	361854.959007	45.145575
3503.271430	361860.865215	45.150580
3502.979158	361829.792353	45.155585
3503.211397	361817.847524	45.160589
3503.221245	361821.357524	45.165594
3502.724826	361822.224951	45.170599
3503.214505	361820.519199	45.175604
3502.960896	361831.729795	45.180609
3502.806568	361829.311622	45.185613
3502.939962	361827.814870	45.190618
3502.874892	361828.843105	45.195623
3503.163229	361829.611905	45.200628
3503.019699	361841.721115	45.205633
3503.138232	361828.700132	45.210637
3503.171978	361832.562582	45.215642
3503.287517	361810.839879	45.220647
3503.106330	361801.835695	45.225652
3503.205957	361802.328991	45.230657
3502.891083	361804.872531	45.235661
3503.243944	361789.829778	45.240666
3502.910174	361801.460175	45.245671
3503.233616	361796.320184	45.250676
3503.012536	361814.981029	45.255681
3503.194306	361812.051708	45.260685
3503.152001	361777.326100	45.265690
3502.957284	361785.041429	45.270695
3503.100375	361778.937593	45.275700
3502.827664	361772.441485	45.280705
3502.839006	361779.360886	45.285709
3502.917548	361776.498772	45.290714
3502.545049	361782.511947	45.295719
3502.718575	361771.899530	45.300724
3502.715316	361779.508255	45.305729
3503.063619	361775.153126	45.310733
3503.269345	361782.576139	45.315738
3503.251437	361787.795346	45.320743
3503.336586	361776.815227	45.325748
3503.469625	361779.008058	45.330753
3503.244607	361774.005666	45.335757
3503.218060	361765.206031	45.340762
3502.914966	361759.986976	45.345767
3503.313136	361758.244800	45.350772
3503.165200	361761.270850	45.355777
3503.224134	361750.294870	45.360781
3503.052905	361760.245652	45.365786
3502.906934	361760.294322	45.370791
3503.226918	361751.567123	45.375796
3503.137729	361750.054668	45.380801
3503.122206	361720.770023	45.385805
3503.160296	361733.181332	45.390810
3503.257774	361725.583443	45.395815
3503.022873	361722.948998	45.400820
3503.005448	361728.066356	45.405825
3503.253598	361727.314808	45.410829
3503.154111	361730.689431	45.415834
3503.043311	361730.401755	45.420839
3503.031731	361695.773010	45.425844
3503.094445	361698.613090	45.430849
3503.059587	361693.580625	45.435853
3503.142976	361698.503931	45.440858
3503.106407	361698.586195	45.445863
3503.184043	361691.424004	45.450868
3502.882755	361709.944901	45.455873
3502.999633	361692.496701	45.460877
3502.858154	361704.020386	45.465882
3502.990633	361705.170060	45.470887
3503.327336	361706.414673	45.475892
3503.374863	361702.005310	45.480897
3503.166412	361681.987699	45.485901
3503.146887	361665.069956	45.490906
3503.017575	361673.919991	45.495911
3503.540446	361671.725530	45.500916
3502.950585	361667.289710	45.505921
3503.006068	361668.477004	45.510925
3503.002611	361675.754991	45.515930
3502.898510	361674.143111	45.520935
3503.070235	361672.563958	45.525940
3502.596431	361668.796808	45.530945
3502.699575	361668.373526	45.535949
3503.003820	361680.971775	45.540954
3503.121842	361678.179750	45.545959
3503.265439	361654.289707	45.550964
3502.734787	361649.030282	45.555969
3502.918944	361647.525498	45.560973
3503.197028	361651.222108	45.565978
3503.096438	361652.484968	45.570983
3503.182542	361637.535232	45.575988
3502.992009	361655.300732	45.580993
3503.226151	361648.037456	45.585997
3503.356952	361654.250970	45.591002
3503.266413	361650.372333	45.596007
3503.095407	361617.117326	45.601012
3502.727195	361624.198537	45.606017
3502.823180	361621.384547	45.611021
3502.842713	361608.328265	45.616026
3502.734467	361618.040113	45.621031
3502.838445	361611.942440	45.626036
3503.214540	361616.539581	45.631041
3503.029395	361615.423970	45.636045
3502.783445	361626.378953	45.641050
3502.877469	361620.231964	45.646055
3502.893805	361621.476339	45.651060
3502.790513	361623.681095	45.656065
3503.038843	361620.766684	45.661069
3503.382185	361627.709952	45.666074
3503.236844	361633.738122	45.671079
3503.466410	361620.801307	45.676084
3503.007016	361622.935139	45.681089
3503.457342	361600.167049	45.686093
3503.107565	361602.639782	45.691098
3503.402616	361599.539867	45.696103
3503.191868	361601.914285	45.701108
3503.152112	361606.195497	45.706113
3503.073514	361603.765339	45.711117
3503.194492	361582.626909	45.716122
3502.982302	361584.034640	45.721127
3503.094848	361569.996727	45.726132
3503.062523	361561.757760	45.731137
3503.314360	361562.354220	45.736141
3503.267007	361576.254897	45.741146
3502.898760	361575.193679	45.746151
3503.527637	361573.135125	45.751156
3503.190236	361579.549898	45.756161
3503.074346	361553.563438	45.761165
3503.059864	361547.917053	45.766170
3502.867975	361547.565861	45.771175
3502.981996	361540.117998	45.776180
3503.274199	361551.420483	45.781185
3503.291024	361548.771675	45.786189
3503.277972	361532.132757	45.791194
3503.219108	361542.040375	45.796199
3503.234178	361523.768519	45.801204
3502.808360	361519.790208	45.806209
3503.085013	361503.588935	45.811213
3503.088277	361511.400233	45.816218
3502.801905	361507.323539	45.821223
3503.064861	361510.615429	45.826228
3503.028746	361512.529673	45.831233
3503.493784	361512.227291	45.836237
3503.065415	361503.287574	45.841242
3502.690874	361516.807430	45.846247
3503.168800	361501.388581	45.851252
3503.070484	361520.640817	45.856257
3503.002698	361513.806933	45.861261
3502.937643	361492.748764	45.866266
3502.938453	361487.888754	45.871271
3503.075319	361476.086144	45.876276
3502.945329	361489.745459	45.881281
3503.015987	361480.548725	45.886285
3503.336928	361476.045224	45.891290
3503.133605	361481.039328	45.896295
3503.406541	361474.253350	45.901300
3502.847954	361486.733614	45.906305
3503.176747	361482.941337	45.911309
3503.126047	361483.000390	45.916314
3503.186149	361465.840980	45.921319
3503.686028	361442.377960	45.926324
3502.938702	361453.997490	45.931329
3503.024404	361447.851795	45.936333
3503.162657	361460.425457	45.941338
3503.045115	361460.266071	45.946343
3503.260627	361450.970094	45.951348
3503.160430	361453.530602	45.956353
3503.135545	361434.018214	45.961357
3502.893864	361437.873352	45.966362
3502.927574	361425.400017	45.971367
3503.517661	361424.747076	45.976372
3503.236542	361427.208963	45.981377
3503.001362	361429.409135	45.986381
3503.589203	361431.530077	45.991386
3503.196398	361426.070717	45.996391
3503.143407	361405.646733	46.001396
3502.967826	361394.453295	46.006401
3502.768707	361392.449305	46.011405
3502.674620	361394.576281	46.016410
3502.982703	361396.945016	46.021415
3503.144350	361396.766935	46.026420
3502.972075	361400.738330	46.031425
3503.238318	361391.485211	46.036429
3502.929172	361399.218693	46.041434
3502.714285	361406.606484	46.046439
3502.958548	361401.657085	46.051444
3503.092389	361403.264566	46.056449
3502.990225	361406.283402	46.061453
3503.205306	361407.725367	46.066458
3502.952110	361400.030197	46.071463
3503.048879	361394.137197	46.076468
3502.718458	361388.718860	46.081473
3502.733455	361374.340077	46.086477
3503.338550	361385.618579	46.091482
3502.844220	361385.213421	46.096487
3502.814097	361370.485538	46.101492
3502.936690	361377.158401	46.106497
3502.805941	361381.250457	46.111501
3502.687508	361379.920732	46.116506
3502.658748	361373.844014	46.121511
3502.825484	361385.497163	46.126516
3502.852010	361397.147032	46.131521
3502.836468	361401.933339	46.136525
3503.072121	361386.705427	46.141530
3502.939102	361389.194792	46.146535
3503.394177	361381.921990	46.151540
3503.076587	361396.145343	46.156545
3503.133513	361392.625048	46.161549
3503.186169	361390.530362	46.166554
3502.974817	361405.169484	46.171559
3503.686370	361393.835789	46.176564
3503.242580	361391.870482	46.181569
3503.264221	361363.012307	46.186573
3502.926256	361372.175284	46.191578
3503.160834	361364.250319	46.196583
3503.034527	361360.351868	46.201588
3502.708566	361368.978597	46.206593
3503.234423	361354.061027	46.211597
3503.170812	361361.704805	46.216602
3502.916995	361354.951200	46.221607
3503.198395	361360.555703	46.226612
3503.110650	361348.661345	46.231617
3502.994345	361336.542493	46.236621
3503.274124	361323.801220	46.241626
3502.936629	361337.925956	46.246631
3503.118387	361331.230709	46.251636
3503.044781	361326.280667	46.256641
3503.045517	361330.988071	46.261645
3503.258334	361332.710295	46.266650
3502.896625	361340.655659	46.271655
3503.438363	361319.959494	46.276660
3502.971330	361316.649258	46.281665
3502.712883	361299.260253	46.286669
3503.206455	361306.154372	46.291674
3503.073184	361303.351163	46.296679
3503.208630	361292.439316	46.301684
3503.123801	361305.124624	46.306689
3503.250841	361300.015631	46.311693
3503.006995	361295.804968	46.316698
3503.262614	361295.713811	46.321703
3503.128119	361291.613086	46.326708
3502.723914	361280.735665	46.331713
3503.096784	361290.218844	46.336717
3503.162381	361275.450353	46.341722
3502.987459	361268.302582	46.346727
3503.085523	361268.643459	46.351732
3502.806746	361271.970125	46.356737
3502.934719	361266.708308	46.361741
3503.090687	361278.286851	46.366746
3502.777687	361279.252514	46.371751
3503.137829	361268.305136	46.376756
3502.903004	361278.164293	46.381761
3503.100381	361278.693031	46.386765
3502.912215	361276.483742	46.391770
3502.943532	361274.570541	46.396775
3503.298297	361280.596024	46.401780
3503.019292	361283.006694	46.406785
3503.294023	361276.652973	46.411789
3502.953816	361262.737440	46.416794
3502.956421	361252.635391	46.421799
3503.667033	361242.726746	46.426804
3503.307399	361243.114540	46.431809
3503.277766	361252.228793	46.436813
3503.404295	361249.155499	46.441818
3503.285310	361234.161724	46.446823
3503.408373	361226.254367	46.451828
3503.060786	361221.627529	46.456833
3503.243343	361220.657336	46.461837
3503.283058	361211.694450	46.466842
3503.064831	361223.510284	46.471847
3503.202697	361197.585291	46.476852
3503.184286	361178.351673	46.481857
3503.099164	361187.067585	46.486861
3502.991354	361176.575850	46.491866
3502.846929	361174.283304	46.496871
3503.163439	361175.861913	46.501876
3502.950263	361178.134954	46.506881
3503.104251	361183.886848	46.511885
3502.996103	361168.865894	46.516890
3502.716321	361190.106247	46.521895
3503.184054	361181.304693	46.526900
3503.294755	361180.778431	46.531905
3502.950061	361176.812711	46.536909
3503.239426	361155.851030	46.541914
3503.090795	361149.844126	46.546919
3503.188896	361143.823658	46.551924
3502.760505	361150.049312	46.556929
3502.979522	361141.745089	46.561933
3503.103437	361138.850319	46.566938
3502.596231	361151.653337	46.571943
3502.887951	361134.686196	46.576948
3502.878508	361140.947396	46.581953
3502.859862	361149.805478	46.586957
3502.988759	361157.011728	46.591962
3502.979034	361149.201687	46.596967
3502.987695	361150.727187	46.601972
3502.981403	361147.802112	46.606977
3503.010794	361150.698384	46.611981
3503.432756	361147.578375	46.616986
3503.000984	361145.687493	46.621991
3503.340475	361125.684798	46.626996
3503.222704	361127.764640	46.632001
3503.022493	361116.066122	46.637005
3503.361892	361122.679299	46.642010
3503.285722	361123.505740	46.647015
3503.028229	361119.169993	46.652020
3502.995647	361117.623123	46.657025
3503.255200	361110.940991	46.662029
3503.275227	361082.006565	46.667034
3502.970242	361081.546023	46.672039
3503.206814	361076.903150	46.677044
3503.344206	361071.868832	46.682049
3502.688935	361078.919172	46.687053
3503.119500	361089.869102	46.692058
3503.068052	361089.801047	46.697063
3503.174409	361092.074464	46.702068
3503.090554	361089.416103	46.707073
3503.077597	361068.222282	46.712077
3503.227743	361053.949263	46.717082
3502.727052	361054.359360	46.722087
3502.895838	361051.559272	46.727092
3503.057236	361056.801102	46.732097
3502.978817	361063.556680	46.737101
3502.999445	361059.558637	46.742106
3502.534726	361056.527917	46.747111
3502.828418	361054.853125	46.752116
3502.855528	361058.055108	46.757121
3502.659265	361059.918354	46.762125
3503.180553	361057.596888	46.767130
3503.264606	361062.774610	46.772135
3503.070409	361061.507744	46.777140
3502.836685	361070.959643	46.782145
3503.234847	361059.141063	46.787149
3503.067971	361053.671385	46.792154
3503.084133	361072.829368	46.797159
3502.855262	361047.191283	46.802164
3502.916268	361037.487081	46.807169
3502.708463	361043.601537	46.812173
3503.065883	361036.776694	46.817178
3503.054389	361029.755722	46.822183
3503.176186	361035.741732	46.827188
3503.032835	361037.494832	46.832193
3503.139833	361029.971663	46.837197
3503.457655	361032.084423	46.842202
3503.078620	361037.284471	46.847207
3503.348114	361038.234383	46.852212
3503.012607	361026.022880	46.857217
3502.794507	361005.497600	46.862221
3502.973288	361009.617088	46.867226
3503.161290	361005.439905	46.872231
3503.184562	361010.041997	46.877236
3502.953503	360999.696936	46.882241
3503.436089	360989.824290	46.887245
3503.187023	360998.566157	46.892250
3503.034766	361000.575120	46.897255
3503.494914	361007.678131	46.902260
3503.416399	360988.733838	46.907265
3503.196774	360975.562519	46.912269
3503.238950	360983.673097	46.917274
3503.071018	360976.651405	46.922279
3503.375392	360975.814621	46.927284
3503.211743	360976.171432	46.932289
3503.274787	360951.403180	46.937293
3503.171367	360950.020177	46.942298
3503.241830	360945.530781	46.947303
3503.284396	360938.552140	46.952308
3503.196765	360940.983461	46.957313
3502.914601	360937.465853	46.962317
3503.057327	360939.479072	46.967322
3503.176135	360924.778396	46.972327
3503.300991	360909.109830	46.977332
3503.044418	360904.010553	46.982337
3503.032019	360900.882865	46.987341
3503.098305	360898.938674	46.992346
3503.007705	360910.912526	46.997351
3503.007144	360904.347826	47.002356
3502.737244	360906.833411	47.007361
3502.975058	360905.981704	47.012365
3503.335359	360907.400725	47.017370
3502.880611	360901.238623	47.022375
3503.393510	360899.020259	47.027380
3503.001301	360894.553117	47.032385
3503.269318	360875.045081	47.037389
3502.930806	360875.582212	47.042394
3502.900766	360872.075628	47.047399
3502.911245	360875.890945	47.052404
3502.917790	360869.274225	47.057409
3502.836657	360876.361051	47.062413
3503.285604	360872.066264	47.067418
3503.007080	360875.011235	47.072423
3503.204890	360875.514463	47.077428
3502.823652	360879.010028	47.082433
3502.954502	360871.279499	47.087437
3502.774664	360870.951842	47.092442
3502.518418	360889.313265	47.097447
3502.578007	360885.538057	47.102452
3502.639111	360881.991618	47.107457
3503.079912	360884.364842	47.112461
3503.065814	360892.637006	47.117466
3503.056687	360893.376515	47.122471
3503.122804	360883.493355	47.127476
3502.956246	360880.695385	47.132481
3502.948740	360880.238699	47.137485
3503.185257	360868.114837	47.142490
3502.810873	360863.746655	47.147495
3502.960470	360857.870683	47.152500
3502.979154	360858.707578	47.157505
3503.180094	360856.360414	47.162509
3503.234546	360849.023643	47.167514
3503.138961	360862.245125	47.172519
3503.281106	360861.357652	47.177524
3503.243290	360858.284870	47.182529
3503.077175	360859.227319	47.187533
3503.008612	360846.006636	47.192538
3502.973961	360834.358211	47.197543
3503.001974	360825.473439	47.202548
3502.963085	360832.222800	47.207553
3502.857483	360822.799350	47.212557
3503.032192	360828.675240	47.217562
3502.827571	360825.552492	47.222567
3503.112722	360821.690726	47.227572
3502.911926	360827.269745	47.232577
3502.822391	360822.500288	47.237581
3502.879355	360832.160731	47.242586
3502.711623	360827.988884	47.247591
3502.606891	360817.878267	47.252596
3502.662310	360832.399052	47.257601
3502.748167	360831.062457	47.262605
3503.330178	360833.184349	47.267610
3503.324940	360834.966511	47.272615
3503.119303	360834.642932	47.277620
3502.984628	360844.053771	47.282625
3503.048983	360839.361767	47.287629
3503.144326	360838.150900	47.292634
3503.065581	360821.445783	47.297639
3503.019877	360812.674445	47.302644
3502.997657	360798.581274	47.307649
3502.939134	360795.995228	47.312653
3503.103164	360803.552214	47.317658
3502.793307	360807.952538	47.322663
3503.116682	360799.758985	47.327668
3503.134146	360804.336569	47.332673
3503.197684	360802.774493	47.337677
3503.320450	360799.727210	47.342682
3503.110663	360808.844585	47.347687
3503.410684	360798.211951	47.352692
3503.388543	360784.627674	47.357697
3503.233929	360774.448597	47.362701
3503.270133	360770.804305	47.367706
3503.233237	360764.448895	47.372711
3503.277269	360757.139202	47.377716
3503.259769	360738.414173	47.382721
3502.938652	360741.594895	47.387725
3503.536022	360724.859186	47.392730
3503.236744	360735.924587	47.397735
3503.016362	360727.053623	47.402740
3503.137195	360743.955978	47.407745
3503.234568	360737.146761	47.412749
3503.171178	360721.762351	47.417754
3502.857466	360705.526917	47.422759
3503.190419	360696.059552	47.427764
3503.074596	360700.861784	47.432769
3503.040203	360693.233688	47.437773
3503.074438	360685.009491	47.442778
3503.105296	360695.768251	47.447783
3503.076785	360689.945862	47.452788
3503.100548	360698.848214	47.457793
3503.087576	360688.392268	47.462797
3502.981806	360710.114236	47.467802
3502.780094	360696.278422	47.472807
3503.035398	360698.553755	47.477812
3503.115814	360674.571426	47.482817
3502.835189	360678.178326	47.487821
3503.244214	360664.398619	47.492826
3503.223833	360668.320614	47.497831
3503.506192	360669.319390	47.502836
3503.377805	360665.421210	47.507841
3503.212373	360663.437308	47.512845
3503.325343	360648.126774	47.517850
3502.845119	360644.004317	47.522855
3503.037345	360629.012040	47.527860
3502.965125	360634.570754	47.532865
3502.682522	360626.676542	47.537869
3503.193381	360631.328810	47.542874
3502.852035	360635.530563	47.547879
3502.756080	360627.250603	47.552884
3502.972278	360633.934218	47.557889
3502.896844	360628.602707	47.562893
3503.292263	360627.242610	47.567898
3503.054896	360644.735991	47.572903
3503.268660	360629.892983	47.577908
3502.943617	360646.585964	47.582913
3502.850671	360630.595502	47.587917
3503.015065	360635.709677	47.592922
3502.895801	360628.705684	47.597927
3503.057643	360620.664867	47.602932
3502.876622	360603.848616	47.607937
3502.773213	360598.038057	47.612941
3503.299095	360598.209518	47.617946
3503.005986	360607.492778	47.622951
3503.237322	360598.804829	47.627956
3503.151674	360606.426767	47.632961
3503.061821	360602.140805	47.637965
3503.320352	360615.917065	47.642970
3503.238594	360613.232900	47.647975
3503.481681	360596.196920	47.652980
3503.222327	360580.181859	47.657985
3503.276865	360569.562541	47.662989
3503.244842	360566.539716	47.667994
3503.222828	360573.566348	47.672999
3503.111842	360571.039476	47.678004
3503.155789	360555.663488	47.683009
3503.082214	360551.298611	47.688013
3502.748408	360541.554946	47.693018
3502.203774	360542.989822	47.698023
3502.688736	360547.162724	47.703028
3503.034978	360578.075515	47.708033
3502.996624	360573.297940	47.713037
3503.126041	360546.305211	47.718042
3503.022432	360557.187044	47.723047
3503.054967	360540.820474	47.728052
3503.062393	360542.956885	47.733057
3502.431170	360548.247749	47.738061
3502.795173	360545.314984	47.743066
3502.845236	360550.930712	47.748071
3503.133332	360547.017567	47.753076
3502.718768	360554.360722	47.758081
3502.473575	360544.628493	47.763085
3502.857374	360546.374604	47.768090
3502.481480	360549.971131	47.773095
3502.891537	360555.428160	47.778100
3503.045200	360554.106283	47.783105
3502.779214	360556.336811	47.788109
3502.925576	360545.906535	47.793114
3502.981970	360553.277013	47.798119
3503.260793	360547.024332	47.803124
3502.995278	360556.735816	47.808129
3502.815734	360557.222371	47.813133
3503.209077	360549.552072	47.818138
3503.122905	360558.599059	47.823143
3503.167474	360561.823760	47.828148
3502.989706	360560.248935	47.833153
3502.995053	360551.036902	47.838157
3502.642610	360565.749480	47.843162
3502.634345	360567.074109	47.848167
3502.875634	360560.954592	47.853172
3503.009209	360562.333133	47.858177
3502.972193	360573.178988	47.863181
3503.046183	360563.345408	47.868186
3502.907516	360566.828090	47.873191
3503.174518	360563.987000	47.878196
3503.091033	360541.226464	47.883201
3503.144336	360525.543639	47.888205
3503.373590	360533.879173	47.893210
3503.071402	360536.115426	47.898215
3503.166770	360527.932429	47.903220
3502.862653	360535.614364	47.908225
3502.749982	360533.749344	47.913229
3503.448996	360533.842541	47.918234
3503.275139	360535.167905	47.923239
3503.241357	360522.832233	47.928244
3503.122403	360514.097867	47.933249
3502.780268	360505.627796	47.938253
3502.641497	360504.224924	47.943258
3502.445669	360514.256193	47.948263
3502.703914	360495.054895	47.953268
3502.830749	360512.948766	47.958273
3502.961418	360504.861966	47.963277
3503.294262	360510.687448	47.968282
3502.922161	360506.013524	47.973287
3502.882457	360512.737614	47.978292
3503.024829	360515.285267	47.983297
3502.715277	360507.878764	47.988301
3503.243152	360517.006797	47.993306
3502.930611	360516.649226	47.998311
3503.412232	360512.018448	48.003316
3503.333220	360517.781815	48.008321
3503.341457	360520.579687	48.013325
3503.209556	360489.226134	48.018330
3502.946488	360473.796877	48.023335
3502.894581	360478.207340	48.028340
3502.799065	360485.652738	48.033345
3503.080786	360484.463287	48.038349
3503.506191	360484.319840	48.043354
3502.859040	360489.155205	48.048359
3503.300557	360480.357668	48.053364
3502.924920	360485.455455	48.058369
3503.095734	360480.212225	48.063373
3503.401986	360474.006089	48.068378
3502.957385	360460.666631	48.073383
3503.195556	360452.969959	48.078388
3502.994847	360455.266508	48.083393
3503.107855	360447.462394	48.088397
3503.281868	360436.111676	48.093402
3502.753765	360453.472972	48.098407
3503.050160	360453.375367	48.103412
3503.083249	360455.711290	48.108417
3503.137810	360455.143005	48.113421
3503.276698	360456.037240	48.118426
3503.010803	360437.325919	48.123431
3502.977791	360413.106934	48.128436
3502.911300	360412.506896	48.133441
3502.850005	360425.468621	48.138445
3503.239630	360415.865011	48.143450
3502.871635	360423.251715	48.148455
3503.029131	360412.972324	48.153460
3503.194932	360416.585000	48.158465
3502.836874	360412.697666	48.163469
3503.072297	360413.576639	48.168474
3502.979847	360417.637277	48.173479
3502.933552	360410.392704	48.178484
3502.612139	360424.108035	48.183489
3502.798693	360425.274638	48.188493
3503.157388	360422.190031	48.193498
3502.849268	360425.852189	48.198503
3503.288407	360419.396024	48.203508
3503.255837	360415.940699	48.208513
3503.119255	360393.570173	48.213517
3503.119028	360397.845244	48.218522
3503.051054	360391.927275	48.223527
3503.155132	360385.676755	48.228532
3503.187784	360388.674340	48.233537
3503.090994	360389.224151	48.238541
3503.253664	360384.974582	48.243546
3503.030714	360396.384235	48.248551
3502.970698	360379.039858	48.253556
3503.136006	360367.639608	48.258561
3503.105656	360351.995398	48.263565
3503.313112	360353.642168	48.268570
3502.884503	360357.679621	48.273575
3503.222577	360359.992776	48.278580
3503.149280	360350.793138	48.283585
3503.015262	360367.405123	48.288589
3503.000090	360360.282851	48.293594
3502.884782	360359.894096	48.298599
3503.022831	360345.037524	48.303604
3503.036566	360355.264706	48.308609
3503.036114	360349.794081	48.313613
3503.141630	360325.604042	48.318618
3502.669638	360328.554187	48.323623
3502.766976	360313.602259	48.328628
3502.903142	360324.293561	48.333633
3502.949885	360336.831096	48.338637
3503.447359	360319.525786	48.343642
3503.009778	360332.114449	48.348647
3503.272374	360320.189891	48.353652
3503.024581	360333.308356	48.358657
3502.986715	360330.311885	48.363661
3503.261501	360320.090268	48.368666
3502.772425	360326.859985	48.373671
3503.014526	360321.401900	48.378676
3503.056381	360313.609014	48.383681
3503.134538	360308.176847	48.388685
3503.284973	360298.509248	48.393690
3502.953141	360298.383737	48.398695
3502.754159	360298.695248	48.403700
3502.916989	360303.657030	48.408705
3502.911585	360296.864000	48.413709
3502.720943	360299.667881	48.418714
3502.694828	360293.997741	48.423719
3503.130362	360297.415106	48.428724
3502.741735	360298.240070	48.433729
3502.720916	360292.111067	48.438733
3503.176186	360293.362418	48.443738
3502.705462	360295.650773	48.448743
3503.032087	360291.985974	48.453748
3502.828133	360299.830232	48.458753
3502.826677	360306.599195	48.463757
3502.727455	360302.009338	48.468762
3502.698186	360308.680915	48.473767
3502.882194	360304.249845	48.478772
3502.747119	360305.441855	48.483777
3502.778861	360304.775392	48.488781
3502.995268	360304.206963	48.493786
3502.817009	360307.161561	48.498791
3502.880907	360303.792759	48.503796
3502.938615	360308.542149	48.508801
3502.846347	360301.610177	48.513805
3503.046479	360306.158929	48.518810
3502.914532	360315.849344	48.523815
3503.145092	360297.619286	48.528820
3503.446974	360318.208256	48.533825
3503.131643	360305.688029	48.538829
3503.088819	360291.292616	48.543834
3503.036663	360275.906286	48.548839
3503.172031	360286.546832	48.553844
3503.180652	360272.372292	48.558849
3503.119895	360273.170865	48.563853
3503.483798	360276.065194	48.568858
3503.129480	360284.162240	48.573863
3503.104707	360282.130638	48.578868
3503.193824	360253.159341	48.583873
3502.846933	360246.852872	48.588877
3502.887668	360242.648015	48.593882
3502.935915	360248.493078	48.598887
3502.875494	360240.589120	48.603892
3503.001311	360244.895169	48.608897
3502.963056	360237.445732	48.613901
3502.672166	360243.369859	48.618906
3502.606310	360242.438922	48.623911
3502.997769	360248.967652	48.628916
3503.128870	360240.855294	48.633921
3503.037738	360255.526653	48.638925
3502.777040	360250.377066	48.643930
3503.082141	360247.173692	48.648935
3503.367679	360250.920126	48.653940
3502.956632	360257.346719	48.658945
3502.957891	360252.435621	48.663949
3503.144440	360251.719237	48.668954
3502.803841	360253.528996	48.673959
3502.971419	360255.080290	48.678964
3503.098021	360236.764861	48.683969
3502.903954	360227.736968	48.688973
3503.030664	360219.345397	48.693978
3502.878115	360217.384885	48.698983
3502.975985	360224.952424	48.703988
3502.974526	360215.334268	48.708993
3502.953454	360229.129400	48.713997
3503.024757	360217.693085	48.719002
3503.102846	360223.711554	48.724007
3503.185784	360226.166836	48.729012
3503.460440	360218.031778	48.734017
3503.240995	360222.239740	48.739021
3503.219132	360201.301401	48.744026
3502.905161	360198.068671	48.749031
3503.253622	360189.056779	48.754036
3503.215056	360194.686561	48.759041
3503.049147	360189.013064	48.764045
3503.243584	360193.995307	48.769050
3502.921535	360197.328887	48.774055
3502.933226	360184.807818	48.779060
3502.945429	360192.312568	48.784065
3502.940556	360199.845462	48.789069
3503.139118	360188.490804	48.794074
3502.815978	360173.936108	48.799079
3503.033738	360153.036200	48.804084
3502.735186	360159.852156	48.809089
3503.011428	360161.920637	48.814093
3502.973191	360162.639314	48.819098
3502.677865	360158.894716	48.824103
3502.712422	360169.093199	48.829108
3502.997319	360165.613110	48.834113
3503.029433	360161.231487	48.839117
3502.862116	360160.214806	48.844122
3502.875724	360169.373320	48.849127
3503.143837	360156.022880	48.854132
3503.156293	360177.013912	48.859137
3502.820262	360169.382530	48.864141
3502.816492	360167.678399	48.869146
3502.697360	360174.974903	48.874151
3502.691954	360171.337144	48.879156
3502.607407	360164.683837	48.884161
3502.633656	360169.819903	48.889165
3502.729633	360176.471696	48.894170
3502.637268	360174.730681	48.899175
3502.938265	360167.660176	48.904180
3503.004537	360176.454121	48.909185
3502.994791	360174.979948	48.914189
3503.253065	360175.906204	48.919194
3503.052705	360183.978926	48.924199
3503.200476	360177.085323	48.929204
3503.102337	360169.594452	48.934209
3503.104097	360178.424041	48.939213
3503.119484	360176.691436	48.944218
3502.787506	360190.026816	48.949223
3503.138807	360173.558832	48.954228
3502.983325	360172.260375	48.959233
3502.918679	360158.148277	48.964237
3503.252118	360147.942796	48.969242
3503.071013	360145.121636	48.974247
3503.173114	360143.757008	48.979252
3503.027490	360138.869121	48.984257
3502.690952	360146.505352	48.989261
3503.109111	360138.423930	48.994266
3502.870954	360140.726415	48.999271
3502.886445	360135.685825	49.004276
3503.137236	360141.015406	49.009281
3502.843618	360146.660072	49.014285
3503.556206	360147.616285	49.019290
3502.731563	360130.774396	49.024295
3502.881862	360126.984787	49.029300
3503.074134	360118.226589	49.034305
3503.191026	360112.101237	49.039309
3503.341695	360113.426196	49.044314
3503.120809	360110.993012	49.049319
3503.273915	360105.472635	49.054324
3503.378411	360104.260303	49.059329
3502.930881	360107.969972	49.064333
3502.872331	360101.643343	49.069338
3503.022380	360108.948190	49.074343
3503.081281	360092.348286	49.079348
3502.837879	360081.165262	49.084353
3502.975015	360071.474274	49.089357
3502.880386	360072.532665	49.094362
3502.748151	360077.617459	49.099367
3502.784096	360069.952698	49.104372
3502.989906	360074.093439	49.109377
3502.745199	360074.971990	49.114381
3503.258585	360077.053875	49.119386
3503.292886	360068.727778	49.124391
3503.371199	360081.972875	49.129396
3503.406421	360081.076846	49.134401
3503.042634	360075.154714	49.139405
3503.094458	360073.060102	49.144410
3502.894711	360059.401915	49.149415
3502.793039	360049.697786	49.154420
3503.025877	360045.666107	49.159425
3502.853442	360046.100652	49.164429
3503.356673	360054.113048	49.169434
3503.198600	360043.501781	49.174439
3502.903416	360052.149328	49.179444
3503.115443	360051.912385	49.184449
3502.962771	360053.921454	49.189453
3503.050411	360049.251137	49.194458
3502.814259	360044.733796	49.199463
3503.125648	360047.763671	49.204468
3503.072709	360049.324391	49.209473
3502.943371	360062.627768	49.214477
3503.257102	360041.305504	49.219482
3502.939509	360031.584618	49.224487
3503.202017	360009.074478	49.229492
3502.992768	360017.377646	49.234497
3502.810833	360017.075760	49.239501
3503.127125	360010.155490	49.244506
3502.867655	360027.728928	49.249511
3502.868182	360014.471646	49.254516
3502.985868	360006.514045	49.259521
3502.907424	360020.241970	49.264525
3503.072063	360014.897881	49.269530
3502.986369	360013.766508	49.274535
3503.226290	360030.523057	49.279540
3503.422873	360027.209595	49.284545
3502.709339	360005.922499	49.289549
3503.005823	359988.038143	49.294554
3502.932401	359980.288875	49.299559
3503.181010	359983.252342	49.304564
3503.299412	359991.859956	49.309569
3503.023657	359985.567652	49.314573
3503.173033	359983.177707	49.319578
3503.071568	359980.725635	49.324583
3502.997842	359984.783350	49.329588
3502.859564	359990.199906	49.334593
3502.866568	359990.453406	49.339597
3502.999760	359986.106679	49.344602
3502.637523	360002.424074	49.349607
3503.283859	359993.441390	49.354612
3503.338389	359964.551725	49.359617
3502.773458	359956.396687	49.364621
3503.102643	359955.784977	49.369626
3502.682719	359958.014425	49.374631
3503.131695	359951.149507	49.379636
3502.925195	359953.396104	49.384641
3502.709786	359956.534719	49.389645
3502.810848	359961.786209	49.394650
3503.016829	359965.036323	49.399655
3502.924500	359954.414642	49.404660
3503.123608	359949.166880	49.409665
3502.892182	359967.117596	49.414669
3502.865043	359957.325327	49.419674
3502.875894	359959.944696	49.424679
3503.172796	359958.447481	49.429684
3502.825061	359959.724013	49.434689
3502.490274	359969.751919	49.439693
3503.056587	359957.830145	49.444698
3503.230445	359955.538111	49.449703
3503.184875	359957.911941	49.454708
3502.986473	359958.605051	49.459713
3503.166290	359961.782964	49.464717
3503.059000	359953.657356	49.469722
3502.719053	359938.723555	49.474727
3503.056999	359920.425483	49.479732
3503.060680	359930.756129	49.484737
3502.538271	359928.777743	49.489741
3502.997074	359929.087043	49.494746
3503.062764	359934.980278	49.499751
3502.996569	359929.519999	49.504756
3502.815846	359943.773036	49.509761
3502.815456	359936.317566	49.514765
3502.888294	359940.835586	49.519770
3502.988027	359937.384754	49.524775
3503.090514	359935.434802	49.529780
3503.202313	359937.656521	49.534785
3502.489041	359942.451503	49.539789
3503.056877	359934.524505	49.544794
3502.976783	359943.188956	49.549799
3502.823446	359942.424520	49.554804
3503.027990	359946.590919	49.559809
3502.805957	359938.330773	49.564813
3503.382170	359935.364421	49.569818
3502.882719	359943.357240	49.574823
3503.211681	359932.999745	49.579828
3503.202469	359919.998437	49.584833
3502.845505	359914.456898	49.589837
3503.022528	359892.240125	49.594842
3502.871857	359907.608046	49.599847
3502.856390	359905.345943	49.604852
3502.742223	359908.901137	49.609857
3502.588711	359903.989026	49.614861
3503.239448	359896.532389	49.619866
3503.011808	359907.484871	49.624871
3503.452317	359894.539685	49.629876
3503.162631	359904.942164	49.634881
3502.744411	359911.522614	49.639885
3502.743962	359902.896631	49.644890
3502.651651	359906.117571	49.649895
3502.925689	359906.481529	49.654900
3502.841030	359907.563793	49.659905
3502.852296	359901.989480	49.664909
3502.899542	359905.570047	49.669914
3502.590897	359913.812610	49.674919
3502.555423	359911.604562	49.679924
3503.053391	359914.350487	49.684929
3502.524943	359920.261321	49.689933
3502.698763	359910.462716	49.694938
3502.798750	359911.668464	49.699943
3502.846795	359915.299796	49.704948
3502.848882	359916.699144	49.709953
3502.776400	359918.873662	49.714957
3503.230686	359920.354192	49.719962
3502.917697	359914.373118	49.724967
3503.081002	359920.505382	49.729972
3503.378180	359928.677606	49.734977
3502.903643	359934.223670	49.739981
3503.104138	359916.787047	49.744986
3502.767056	359926.509973	49.749991
3503.000851	359921.027710	49.754996
3503.037155	359936.773197	49.760001
3502.924396	359913.609855	49.765005
3503.113190	359888.057791	49.770010
3502.709945	359892.752869	49.775015
3502.912233	359892.771926	49.780020
3503.077627	359891.957097	49.785025
3502.974127	359901.414084	49.790029
3502.673314	359894.006104	49.795034
3502.852467	359896.929666	49.800039
3503.107940	359890.120779	49.805044
3503.143160	359898.054519	49.810049
3502.791212	359902.563364	49.815053
3502.580862	359897.405778	49.820058
3502.690959	359905.989275	49.825063
3502.790772	359903.047349	49.830068
3502.904691	359901.426386	49.835073
3502.848254	359914.591048	49.840077
3503.024998	359902.883529	49.845082
3503.094658	359898.979421	49.850087
3503.218392	359906.441136	49.855092
3503.180718	359899.373245	49.860097
3502.998236	359904.313325	49.865101
3503.118197	359899.841452	49.870106
3502.946416	359904.957963	49.875111
3502.921472	359889.948898	49.880116
3502.936457	359888.827051	49.885121
3502.676126	359891.947327	49.890125
3502.999904	359888.181163	49.895130
3503.029799	359884.639585	49.900135
3503.322220	359875.432927	49.905140
3503.167272	359879.630722	49.910145
3502.602704	359880.381726	49.915149
3502.948937	359873.482149	49.920154
3502.753165	359885.320208	49.925159
3502.618362	359874.756117	49.930164
3502.835947	359871.770123	49.935169
3502.768756	359879.796395	49.940173
3503.126069	359873.760232	49.945178
3502.677195	359871.312189	49.950183
3502.931384	359873.384169	49.955188
3502.871199	359881.511118	49.960193
3503.056702	359877.334232	49.965197
3503.250473	359879.542995	49.970202
3502.950539	359886.562776	49.975207
3503.052188	359882.729947	49.980212
3503.245807	359885.167748	49.985217
3503.194246	359884.641680	49.990221
3503.280902	359872.006893	49.995226
3502.813673	359855.133844	50.000231
3502.781027	359836.665318	50.005236
3502.980689	359838.771367	50.010241
3502.588741	359841.479872	50.015245
3503.304296	359832.893351	50.020250
3503.235978	359840.105534	50.025255
3503.241391	359836.466039	50.030260
3503.233138	359844.075861	50.035265
3502.442652	359846.720145	50.040269
3502.882138	359842.884793	50.045274
3502.864591	359840.623015	50.050279
3503.133422	359840.682444	50.055284
3503.330250	359846.453172	50.060289
3502.882325	359849.501325	50.065293
3503.395225	359849.165922	50.070298
3502.888406	359828.609445	50.075303
3502.770695	359817.991747	50.080308
3503.072062	359812.880480	50.085313
3503.060387	359811.177586	50.090317
3503.151577	359811.214208	50.095322
3503.165340	359811.313964	50.100327
3503.025484	359807.773772	50.105332
3503.011426	359814.722919	50.110337
3503.121836	359812.746263	50.115341
3503.194402	359812.633153	50.120346
3503.053015	359814.564109	50.125351
3502.922107	359803.770372	50.130356
3503.038111	359787.644810	50.135361
3503.022540	359780.497069	50.140365
3502.913503	359780.692577	50.145370
3503.068703	359778.301701	50.150375
3503.038921	359776.296315	50.155380
3503.007286	359789.075400	50.160385
3502.718286	359785.202541	50.165389
3503.269186	359778.983083	50.170394
3502.923903	359796.086696	50.175399
3502.849602	359785.258559	50.180404
3503.145068	359787.196787	50.185409
3503.032532	359785.128148	50.190413
3503.122761	359787.251500	50.195418
3502.986493	359787.731221	50.200423
3502.925757	359774.000084	50.205428
3503.360027	359774.287817	50.210433
3502.860723	359754.951533	50.215437
3503.069908	359740.108975	50.220442
3502.926029	359755.272302	50.225447
3502.901972	359747.744206	50.230452
3503.144545	359752.286301	50.235457
3502.865964	359754.060827	50.240461
3503.021802	359750.702896	50.245466
3502.963766	359753.053260	50.250471
3503.150224	359742.387456	50.255476
3503.040266	359743.346494	50.260481
3503.088305	359764.637433	50.265485
3503.532101	359747.340405	50.270490
3503.251609	359745.705455	50.275495
3502.864873	359722.865245	50.280500
3503.321663	359711.724110	50.285505
3503.277356	359717.227625	50.290509
3503.291423	359713.713983	50.295514
3502.813468	359723.179314	50.300519
3503.044410	359713.193516	50.305524
3502.965778	359719.643964	50.310529
3503.000258	359714.829342	50.315533
3502.668158	359693.049217	50.320538
3502.746131	359701.765060	50.325543
3502.881209	359710.319195	50.330548
3503.122049	359712.444186	50.335553
3502.817905	359713.866509	50.340557
3503.164823	359687.017033	50.345562
3502.785857	359695.270751	50.350567
3502.670266	359678.291153	50.355572
3502.894950	359676.525440	50.360577
3502.426997	359694.793560	50.365581
3502.827531	359700.175854	50.370586
3502.844773	359713.914183	50.375591
3502.968590	359724.404003	50.380596
3502.971102	359713.182013	50.385601
3502.658692	359696.869693	50.390605
3503.112403	359688.502668	50.395610
3502.812084	359709.975938	50.400615
3502.998944	359684.831210	50.405620
3503.008936	359697.578291	50.410625
3502.707284	359685.768231	50.415629
3502.851988	359687.933868	50.420634
3502.790672	359707.231877	50.425639
3503.116679	359692.523511	50.430644
3502.815215	359685.471848	50.435649
3503.268587	359697.792584	50.440653
3503.399424	359683.776671	50.445658
3503.032988	359695.107390	50.450663
3502.894287	359696.121866	50.455668
3503.196820	359693.656799	50.460673
3503.217056	359702.229093	50.465677
3502.953511	359694.458945	50.470682
3502.933585	359686.344925	50.475687
3503.115040	359660.564886	50.480692
3503.141206	359668.347418	50.485697
3502.856715	359670.250112	50.490701
3503.129574	359653.488999	50.495706
3502.742581	359662.558268	50.500711
3502.800722	359667.282207	50.505716
3503.281626	359664.992507	50.510721
3503.091545	359663.165137	50.515725
3503.190056	359660.935895	50.520730
3502.642159	359643.363033	50.525735
3502.923880	359616.956410	50.530740
3502.709673	359605.666875	50.535745
3502.424234	359560.468822	50.540749
3502.661461	359506.918066	50.545754
3502.273402	359469.064665	50.550759
3501.901129	359399.731691	50.555764
3501.958392	359331.399452	50.560769
3501.314210	359256.740088	50.565773
3501.439882	359157.250429	50.570778
3501.048905	359082.219960	50.575783
3501.023384	358980.463663	50.580788
3500.370940	358883.030400	50.585793
3500.096747	358770.370958	50.590797
3499.734382	358657.038136	50.595802
3499.539698	358536.120859	50.600807
3499.411167	358415.828995	50.605812
3498.992245	358284.182550	50.610817
3498.266323	358144.288588	50.615821
3498.000539	358001.878565	50.620826
3497.615365	357858.189204	50.625831
3496.979785	357721.995033	50.630836
3496.568209	357560.954016	50.635841
3495.615152	357414.121349	50.640845
3495.464236	357245.811056	50.645850
3495.031228	357098.971577	50.650855
3494.384506	356939.339885	50.655860
3494.093169	356772.627944	50.660865
3493.193199	356602.754366	50.665869
3492.666043	356430.276486	50.670874
3492.396072	356273.433259	50.675879
3492.074991	356095.068629	50.680884
3491.448253	355914.639504	50.685889
3490.527963	355748.481674	50.690893
3490.307779	355558.443938	50.695898
3489.501046	355381.604129	50.700903
3488.394404	355200.942960	50.705908
3488.226312	355017.078935	50.710913
3487.551297	354840.496358	50.715917
3487.273724	354653.594502	50.720922
3486.179272	354467.101060	50.725927
3485.697963	354293.285341	50.730932
3485.363547	354098.603097	50.735937
3484.519200	353915.147442	50.740941
3483.747076	353716.817403	50.745946
3483.059378	353526.718821	50.750951
3482.352027	353337.411582	50.755956
3481.978257	353150.061421	50.760961
3481.079112	352960.172354	50.765965
3480.751968	352774.035054	50.770970
3480.307021	352591.173285	50.775975
3479.580878	352392.551010	50.780980
3478.788089	352186.507151	50.785985
3477.931414	352006.049850	50.790989
3477.572902	351798.128868	50.795994
3477.124037	351613.660989	50.800999
3476.026632	351421.074576	50.806004
3475.704258	351223.325753	50.811009
3475.036908	351018.860922	50.816013
3474.545498	350822.613479	50.821018
3473.543422	350629.321990	50.826023
3472.967268	350428.505396	50.831028
3472.245188	350219.388706	50.836033
3471.389433	350028.158907	50.841037
3470.962737	349834.722711	50.846042
3470.231180	349637.465464	50.851047
3469.679131	349435.445198	50.856052
3468.933657	349235.338171	50.861057
3468.246359	349046.038060	50.866061
3467.730478	348839.021417	50.871066
3466.988062	348641.864128	50.876071
3466.471274	348442.532525	50.881076
3465.966444	348242.103891	50.886081
3465.056182	348048.457933	50.891085
3464.586202	347834.940079	50.896090
3463.947439	347632.010698	50.901095
3463.255181	347427.587369	50.906100
3462.601241	347236.952342	50.911105
3461.969533	347028.394737	50.916109
3461.115672	346819.922398	50.921114
3460.124262	346612.540050	50.926119
3459.289741	346415.745870	50.931124
3459.330897	346213.009341	50.936129
3458.503724	346015.805384	50.941133
3457.704889	345800.881088	50.946138
3457.346440	345605.586937	50.951143
3456.301058	345406.302809	50.956148
3455.829437	345196.593309	50.961153
3454.663632	344999.566704	50.966157
3454.222838	344791.683505	50.971162
3453.318374	344607.671796	50.976167
3453.242815	344401.562108	50.981172
3452.520757	344191.354089	50.986177
3451.703888	344006.970305	50.991181
3451.197746	343796.039494	50.996186
3450.481673	343591.275499	51.001191
3449.618150	343381.825146	51.006196
3448.819301	343190.334346	51.011201
3448.127513	342996.687865	51.016205
3447.662575	342786.994232	51.021210
3446.958343	342594.570226	51.026215
3446.167168	342387.701305	51.031220
3445.868085	342183.808396	51.036225
3445.045999	341983.459316	51.041229
3444.152674	341782.051751	51.046234
3443.534416	341583.527315	51.051239
3442.961348	341379.547777	51.056244
3442.114314	341174.185417	51.061249
3441.218465	340988.608554	51.066253
3440.703536	340787.290634	51.071258
3439.737240	340590.014427	51.076263
3439.251175	340404.829216	51.081268
3438.636238	340204.467070	51.086273
3437.817390	340008.743939	51.091277
3437.223416	339811.915515	51.096282
3436.136614	339624.633837	51.101287
3435.862074	339430.859280	51.106292
3435.389195	339237.064584	51.111297
3434.476705	339048.429953	51.116301
3434.452616	338853.850367	51.121306
3433.615698	338656.573127	51.126311
3432.648879	338457.661189	51.131316
3432.339185	338251.644325	51.136321
3431.456433	338062.722084	51.141325
3430.775701	337858.162728	51.146330
3429.940433	337662.205916	51.151335
3429.705188	337458.694935	51.156340
3428.978191	337261.879745	51.161345
3428.392716	337063.590568	51.166349
3427.448070	336854.462194	51.171354
3426.665226	336666.054717	51.176359
3425.746499	336461.146801	51.181364
3425.293862	336258.175635	51.186369
3424.556612	336081.978544	51.191373
3424.046931	335881.026345	51.196378
3423.261778	335688.594285	51.201383
3422.656797	335494.707589	51.206388
3421.750282	335292.136225	51.211393
3421.035652	335099.971367	51.216397
3420.404257	334900.766597	51.221402
3419.831665	334706.337929	51.226407
3419.000018	334511.949677	51.231412
3418.716741	334330.864801	51.236417
3417.538557	334136.784866	51.241421
3417.162383	333942.119322	51.246426
3416.308270	333745.263077	51.251431
3415.997439	333549.873286	51.256436
3415.282733	333355.361470	51.261441
3414.478603	333165.318392	51.266445
3414.012275	332976.239701	51.271450
3413.740011	332780.383430	51.276455
3412.578832	332585.812806	51.281460
3412.355760	332384.092294	51.286465
3411.490505	332195.354651	51.291469
3410.969231	331985.609902	51.296474
3409.906419	331791.963521	51.301479
3409.032674	331585.251980	51.306484
3408.470964	331397.737167	51.311489
3407.722899	331212.899036	51.316493
3407.291225	331005.377635	51.321498
3406.590044	330819.436371	51.326503
3405.631093	330627.221614	51.331508
3405.304338	330424.519154	51.336513
3404.525930	330254.194970	51.341517
3403.768075	330048.326369	51.346522
3402.838681	329861.756852	51.351527
3402.407833	329665.611766	51.356532
3401.825374	329475.574894	51.361537
3401.208175	329283.378998	51.366541
3400.658816	329098.631470	51.371546
3399.787145	328901.484817	51.376551
3398.696623	328709.667832	51.381556
3398.640543	328503.785867	51.386561
3397.749985	328330.241710	51.391565
3397.077654	328127.765941	51.396570
3396.290729	327944.606233	51.401575
3395.593950	327755.881604	51.406580
3395.047491	327555.446674	51.411585
3394.030559	327381.945836	51.416589
3393.705385	327190.767839	51.421594
3393.316637	327002.069054	51.426599
3392.296865	326803.922078	51.431604
3391.452414	326626.726045	51.436609
3390.598513	326434.254986	51.441613
3390.062831	326237.684953	51.446618
3389.678041	326065.685252	51.451623
3388.912317	325878.825644	51.456628
3388.655688	325683.330378	51.461633
3387.549707	325499.349812	51.466637
3387.196047	325319.247158	51.471642
3386.731139	325115.610624	51.476647
3385.770834	324933.260682	51.481652
3385.001392	324735.069030	51.486657
3383.978992	324552.982673	51.491661
3383.788527	324352.992664	51.496666
3382.609991	324171.948597	51.501671
3382.018073	323988.850867	51.506676
3381.693276	323793.387353	51.511681
3380.518791	323616.313365	51.516685
3380.138589	323445.605976	51.521690
3379.604606	323252.211181	51.526695
3378.855206	323064.655182	51.531700
3378.324187	322878.744677	51.536705
3377.711178	322695.520180	51.541709
3376.991689	322496.042287	51.546714
3376.173495	322321.429943	51.551719
3375.408448	322134.943771	51.556724
3375.013769	321945.266850	51.561729
3374.128814	321759.104377	51.566733
3373.515595	321576.234014	51.571738
3373.159892	321387.339034	51.576743
3372.591881	321200.845176	51.581748
3371.718024	321011.751265	51.586753
3370.973977	320820.574008	51.591757
3370.522319	320624.054012	51.596762
3369.345868	320440.684770	51.601767
3368.921964	320258.800243	51.606772
3368.450013	320060.296188	51.611777
3367.678636	319876.556193	51.616781
3366.701786	319696.845895	51.621786
3366.314222	319510.294541	51.626791
3365.571091	319326.599902	51.631796
3365.155998	319133.279164	51.636801
3364.125912	318954.288787	51.641805
3363.915051	318768.904729	51.646810
3363.241194	318579.137591	51.651815
3362.336431	318384.084911	51.656820
3361.712417	318198.153973	51.661825
3361.122455	318012.268210	51.666829
3360.304305	317825.170502	51.671834
3359.322985	317640.364423	51.676839
3359.124829	317454.008203	51.681844
3358.552852	317266.081125	51.686849
3357.415873	317081.018505	51.691853
3357.094423	316891.319600	51.696858
3356.172990	316705.229120	51.701863
3355.531550	316524.975973	51.706868
3355.239012	316326.741279	51.711873
3354.182522	316138.150245	51.716877
3353.734196	315963.772989	51.721882
3352.996742	315772.864580	51.726887
3352.193532	315592.813577	51.731892
3351.295695	315406.920649	51.736897
3350.642061	315225.037438	51.741901
3350.010208	315054.863640	51.746906
3349.642302	314865.702979	51.751911
3348.423535	314681.285448	51.756916
3348.313844	314495.673627	51.761921
3347.465094	314319.192491	51.766925
3346.693805	314144.353943	51.771930
3345.969164	313949.213149	51.776935
3345.230028	313768.486774	51.781940
3345.011697	313593.865417	51.786945
3344.109546	313419.632035	51.791949
3343.634843	313230.510782	51.796954
3343.088806	313053.775946	51.801959
3342.198402	312868.692180	51.806964
3341.332259	312685.896021	51.811969
3340.647846	312500.371622	51.816973
3340.171492	312318.811863	51.821978
3339.631183	312147.905930	51.826983
3338.983522	311964.004519	51.831988
3338.547619	311780.349415	51.836993
3337.360239	311595.768836	51.841997
3336.605458	311405.466454	51.847002
3336.097265	311229.995926	51.852007
3335.532208	311052.547898	51.857012
3335.007642	310859.712676	51.862017
3333.986656	310676.784935	51.867021
3333.721778	310495.927255	51.872026
3332.809769	310314.102140	51.877031
3332.223168	310137.216330	51.882036
3331.704674	309941.501119	51.887041
3330.812057	309764.943262	51.892045
3330.081785	309591.084185	51.897050
3329.280978	309401.346010	51.902055
3328.525978	309232.863383	51.907060
3328.263134	309060.279231	51.912065
3327.424518	308871.819441	51.917069
3326.580694	308673.632591	51.922074
3326.136945	308515.794990	51.927079
3325.287448	308328.736654	51.932084
3325.105229	308146.690952	51.937089
3324.108347	307973.330099	51.942093
3323.407827	307785.305171	51.947098
3322.914584	307615.607524	51.952103
3321.962225	307433.988185	51.957108
3321.693590	307245.028321	51.962113
3320.637053	307073.967534	51.967117
3320.054258	306895.192005	51.972122
3319.301812	306720.415650	51.977127
3318.760174	306544.128724	51.982132
3318.271611	306356.042701	51.987137
3317.336599	306180.301351	51.992141
3316.765494	306012.167298	51.997146
3316.279795	305829.198622	52.002151
3315.562965	305648.965599	52.007156
3315.043870	305465.619726	52.012161
3314.096312	305288.784167	52.017165
3313.683968	305107.992946	52.022170
3312.879798	304919.751102	52.027175
3312.437686	304740.008196	52.032180
3311.955466	304548.022395	52.037185
3311.088430	304374.483466	52.042189
3310.391451	304191.291360	52.047194
3309.506332	304006.142443	52.052199
3308.837276	303825.975877	52.057204
3308.177780	303636.996381	52.062209
3307.114809	303480.906006	52.067213
3306.912908	303285.945577	52.072218
3305.960533	303115.881983	52.077223
3305.178363	302946.631645	52.082228
3304.932067	302771.108102	52.087233
3304.254035	302586.332070	52.092237
3303.388816	302400.057455	52.097242
3303.145890	302221.324006	52.102247
3302.177596	302042.068435	52.107252
3301.460645	301868.451850	52.112257
3300.881839	301681.901851	52.117261
3300.007463	301501.357480	52.122266
3299.302618	301335.225454	52.127271
3298.736880	301155.956106	52.132276
3298.445720	300976.057395	52.137281
3297.559228	300800.683798	52.142285
3296.715262	300621.305060	52.147290
3296.184702	300448.548742	52.152295
3295.581140	300269.971976	52.157300
3295.264421	300082.869307	52.162305
3294.438498	299915.201507	52.167309
3293.522168	299723.405582	52.172314
3293.109037	299546.453231	52.177319
3292.031726	299366.982703	52.182324
3291.675830	299187.652529	52.187329
3290.927536	299010.650771	52.192333
3290.235289	298821.110371	52.197338
3289.517529	298646.319006	52.202343
3288.794002	298465.798370	52.207348
3288.377404	298292.869014	52.212353
3287.659373	298120.394641	52.217357
3286.590338	297936.642911	52.222362
3286.048316	297763.707416	52.227367
3285.183392	297587.894151	52.232372
3285.143134	297411.160788	52.237377
3284.081438	297233.315496	52.242381
3283.293643	297059.603276	52.247386
3282.631449	296883.757271	52.252391
3282.319006	296712.898228	52.257396
3281.757984	296531.025690	52.262401
3280.947886	296360.295992	52.267405
3280.257428	296175.693159	52.272410
3279.323615	295995.458046	52.277415
3278.682710	295822.001604	52.282420
3278.319533	295641.192021	52.287425
3277.538613	295475.372086	52.292429
3276.806678	295298.899005	52.297434
3276.321767	295123.201641	52.302439
3275.720231	294937.946918	52.307444
3274.959949	294759.134877	52.312449
3273.985231	294591.231109	52.317453
3273.677308	294415.454214	52.322458
3273.075098	294235.648967	52.327463
3272.198826	294060.190896	52.332468
3271.841986	293877.366861	52.337473
3270.864748	293716.466316	52.342477
3270.409192	293525.278856	52.347482
3269.699251	293344.496693	52.352487
3269.257044	293170.217147	52.357492
3268.515420	292992.775943	52.362497
3267.217995	292824.361596	52.367501
3266.850900	292638.227412	52.372506
3266.196773	292463.522445	52.377511
3265.547903	292284.003163	52.382516
3264.708151	292115.592307	52.387521
3263.889107	291951.049120	52.392525
3263.069122	291767.176112	52.397530
3262.389585	291600.802425	52.402535
3261.799365	291425.577250	52.407540
3261.406831	291259.769154	52.412545
3260.406543	291094.286307	52.417549
3260.399836	290918.357246	52.422554
3259.670489	290750.717502	52.427559
3258.881005	290588.002423	52.432564
3258.387862	290407.285654	52.437569
3257.579344	290232.527161	52.442573
3257.003608	290052.383511	52.447578
3256.116964	289891.567994	52.452583
3255.453377	289704.867344	52.457588
3255.113779	289532.504594	52.462593
3253.792221	289371.935861	52.467597
3253.661581	289187.493591	52.472602
3253.007003	289014.849283	52.477607
3252.024587	288841.900190	52.482612
3251.356337	288674.886233	52.487617
3250.426714	288501.240962	52.492621
3250.057784	288328.678408	52.497626
3249.577883	288159.418670	52.502631
3248.713798	287984.642155	52.507636
3248.381699	287812.277235	52.512641
3247.684127	287644.426928	52.517645
3247.127919	287465.602963	52.522650
3246.207994	287290.529297	52.527655
3245.380556	287126.952420	52.532660
3244.914367	286948.903447	52.537665
3243.730238	286782.224812	52.542669
3243.531213	286598.250290	52.547674
3242.482567	286432.033948	52.552679
3241.945019	286266.500710	52.557684
3241.699535	286087.499542	52.562689
3240.500201	285930.067815	52.567693
3240.184112	285757.393733	52.572698
3239.719569	285586.322081	52.577703
3238.737494	285416.172681	52.582708
3237.997162	285242.113814	52.587713
3237.377698	285074.912133	52.592717
3236.995324	284898.886380	52.597722
3236.158297	284729.808875	52.602727
3235.455748	284558.290556	52.607732
3235.124786	284380.499157	52.612737
3234.043971	284217.215821	52.617741
3233.331752	284047.787223	52.622746
3232.485351	283876.597021	52.627751
3231.582681	283710.152739	52.632756
3231.381234	283548.767494	52.637761
3230.714647	283376.275256	52.642765
3229.933208	283204.819858	52.647770
3229.290759	283047.349922	52.652775
3228.485271	282883.411341	52.657780
3228.047215	282706.884213	52.662785
3227.233888	282552.319075	52.667789
3226.563494	282385.633870	52.672794
3226.182798	282219.081058	52.677799
3225.433014	282055.693721	52.682804
3225.111221	281884.190656	52.687809
3224.011597	281716.834594	52.692813
3223.466472	281544.679127	52.697818
3222.962757	281378.349297	52.702823
3222.101112	281202.067022	52.707828
3221.285610	281031.991663	52.712833
3220.855336	280878.944536	52.717837
3220.209031	280703.493986	52.722842
3219.836498	280526.497449	52.727847
3218.708472	280363.882660	52.732852
3218.010988	280193.661095	52.737857
3217.355197	280033.238201	52.742861
3216.660279	279854.738957	52.747866
3216.267010	279689.053456	52.752871
3215.300565	279528.857900	52.757876
3214.751983	279362.636611	52.762881
3214.263828	279191.031913	52.767885
3213.290484	279025.590889	52.772890
3212.708391	278860.469960	52.777895
3212.136128	278691.781882	52.782900
3211.422894	278529.763325	52.787905
3210.500746	278367.293904	52.792909
3210.053528	278191.556704	52.797914
3209.716368	278031.465114	52.802919
3208.796392	277866.983289	52.807924
3207.834436	277693.161195	52.812929
3207.122721	277531.396968	52.817933
3206.780040	277371.509931	52.822938
3206.098716	277210.250234	52.827943
3205.433051	277053.572355	52.832948
3205.024292	276880.604987	52.837953
3204.044415	276713.229144	52.842957
3203.354338	276541.987179	52.847962
3202.876804	276383.929668	52.852967
3202.224896	276218.386565	52.857972
3201.735408	276052.664946	52.862977
3200.678668	275874.120602	52.867981
3200.123120	275716.049942	52.872986
3199.440376	275550.715445	52.877991
3198.889898	275390.631975	52.882996
3198.552890	275216.532579	52.888001
3197.607302	275047.597688	52.893005
3197.057471	274876.486301	52.898010
3196.155725	274710.320531	52.903015
3195.330246	274542.436315	52.908020
3195.033720	274381.854241	52.913025
3193.888550	274216.643864	52.918029
3193.440632	274042.078142	52.923034
3192.851175	273878.842789	52.928039
3191.951937	273716.471449	52.933044
3191.477271	273551.002201	52.938049
3190.423300	273390.412685	52.943053
3189.990375	273217.678367	52.948058
3189.292511	273057.108933	52.953063
3188.462611	272907.944769	52.958068
3188.016785	272740.306211	52.963073
3187.251352	272586.547567	52.968077
3186.753542	272421.591447	52.973082
3186.329922	272259.934493	52.978087
3185.406745	272097.439744	52.983092
3185.026380	271931.879325	52.988097
3184.181782	271766.672538	52.993101
3183.216650	271604.260897	52.998106
3182.912934	271446.456265	53.003111
3182.051311	271280.029762	53.008116
3181.466799	271106.250024	53.013121
3180.964840	270946.362964	53.018125
3180.110810	270781.030482	53.023130
3179.447701	270616.941235	53.028135
3178.650445	270453.637295	53.033140
3178.161935	270299.172975	53.038145
3177.453327	270133.613857	53.043149
3176.930913	269970.164649	53.048154
3176.265104	269807.680493	53.053159
3175.518169	269646.762775	53.058164
3174.636606	269479.193703	53.063169
3173.986202	269310.365615	53.068173
3173.285416	269153.744847	53.073178
3172.755609	268993.353222	53.078183
3171.959210	268836.365634	53.083188
3171.567477	268672.386683	53.088193
3170.762589	268513.184779	53.093197
3170.089224	268353.401804	53.098202
3169.941813	268189.588067	53.103207
3169.083144	268027.007528	53.108212
3168.608782	267851.173681	53.113217
3167.522642	267696.880939	53.118221
3167.315072	267527.397501	53.123226
3165.944914	267364.592479	53.128231
3165.118844	267207.992055	53.133236
3164.527006	267039.792056	53.138241
3163.734641	266883.695763	53.143245
3163.195988	266728.603566	53.148250
3162.783542	266572.167102	53.153255
3161.919340	266420.564723	53.158260
3161.290693	266255.350598	53.163265
3160.790506	266099.208328	53.168269
3160.353686	265932.563217	53.173274
3159.391977	265775.322561	53.178279
3158.774218	265621.924154	53.183284
3158.208899	265452.574474	53.188289
3157.461321	265293.440940	53.193293
3156.610473	265133.610703	53.198298
3156.161878	264979.803742	53.203303
3155.209732	264816.296792	53.208308
3154.667174	264650.840459	53.213313
3153.941114	264505.660323	53.218317
3153.388036	264352.379505	53.223322
3152.721738	264191.476261	53.228327
3152.084198	264037.928789	53.233332
3151.479911	263864.180001	53.238337
3150.512120	263716.262417	53.243341
3150.039971	263561.721193	53.248346
3149.575310	263409.038012	53.253351
3148.867852	263246.409885	53.258356
3148.125345	263081.571672	53.263361
3147.599954	262931.648852	53.268365
3147.048092	262755.829422	53.273370
3146.238875	262606.588363	53.278375
3145.247845	262446.170275	53.283380
3144.770574	262285.594561	53.288385
3144.183216	262126.488017	53.293389
3143.620720	261968.065253	53.298394
3143.030353	261812.270167	53.303399
3142.192894	261653.687335	53.308404
3141.526572	261479.720416	53.313409
3140.532167	261332.648574	53.318413
3140.239043	261168.427879	53.323418
3139.151909	261014.774716	53.328423
3138.520396	260866.041212	53.333428
3138.288161	260705.121953	53.338433
3137.405469	260543.465289	53.343437
3137.025370	260389.089350	53.348442
3135.958897	260243.150055	53.353447
3135.563062	260079.939489	53.358452
3135.124746	259920.122945	53.363457
3133.998694	259760.135189	53.368461
3133.524514	259606.895162	53.373466
3132.942021	259448.680713	53.378471
3132.217437	259290.157767	53.383476
3131.479967	259129.166603	53.388481
3130.740638	258976.656538	53.393485
3130.207607	258809.521006	53.398490
3129.339861	258661.768421	53.403495
3128.819958	258513.094979	53.408500
3128.551420	258346.248981	53.413505
3127.426798	258187.331632	53.418509
3126.991272	258040.937201	53.423514
3126.214809	257867.423037	53.428519
3125.393652	257726.437997	53.433524
3125.037457	257552.883022	53.438529
3124.233876	257406.649105	53.443533
3123.837833	257245.707035	53.448538
3123.035316	257086.561189	53.453543
3122.363562	256930.425375	53.458548
3121.646934	256757.437397	53.463553
3120.576829	256609.667203	53.468557
3120.038527	256461.278132	53.473562
3119.658554	256291.726261	53.478567
3118.728940	256155.496288	53.483572
3118.314911	255994.812649	53.488577
3117.671395	255836.788574	53.493581
3117.136997	255683.764389	53.498586
3116.249239	255525.626400	53.503591
3115.511911	255365.834825	53.508596
3115.311808	255212.885416	53.513601
3114.283851	255054.133299	53.518605
3113.560745	254889.781230	53.523610
3112.845056	254731.794894	53.528615
3111.949761	254585.755697	53.533620
3111.581646	254420.278216	53.538625
3110.558726	254274.055712	53.543629
3110.102573	254118.168022	53.548634
3109.458976	253965.366163	53.553639
3108.816164	253820.178925	53.558644
3107.751910	253664.973585	53.563649
3107.324704	253521.178601	53.568653
3106.828608	253365.501584	53.573658
3106.375082	253205.030183	53.578663
3105.583506	253059.026669	53.583668
3104.979048	252897.866350	53.588673
3104.275765	252752.587645	53.593677
3103.790123	252588.632910	53.598682
3102.883510	252439.108215	53.603687
3101.917877	252286.638841	53.608692
3101.496569	252125.144624	53.613697
3100.618708	251979.843242	53.618701
3100.384230	251824.355342	53.623706
3099.415140	251665.214780	53.628711
3098.768088	251513.968989	53.633716
3098.396339	251354.072039	53.638721
3097.650243	251208.368450	53.643725
3096.921164	251044.428223	53.648730
3096.340617	250899.895626	53.653735
3095.378870	250745.389674	53.658740
3095.223835	250579.525455	53.663745
3094.165845	250427.581681	53.668749
3093.498557	250286.934252	53.673754
3092.777896	250127.246495	53.678759
3092.198591	249977.723087	53.683764
3091.409198	249820.389421	53.688769
3090.903786	249673.910566	53.693773
3090.116606	249520.778793	53.698778
3089.589139	249373.794378	53.703783
3088.841376	249223.789011	53.708788
3088.288371	249064.610572	53.713793
3087.390412	248921.632491	53.718797
3086.492218	248773.994260	53.723802
3086.362536	248621.268626	53.728807
3085.777945	248472.893461	53.733812
3085.371513	248307.809918	53.738817
3084.105207	248151.801259	53.743821
3083.287124	248003.463509	53.748826
3082.712246	247865.528500	53.753831
3081.674967	247710.018838	53.758836
3081.504440	247556.358501	53.763841
3080.763065	247420.003685	53.768845
3080.019007	247272.011474	53.773850
3079.862737	247125.658063	53.778855
3079.096452	246978.051657	53.783860
3078.319432	246825.353924	53.788865
3077.310904	246674.093619	53.793869
3077.103620	246517.078704	53.798874
3076.396960	246363.351695	53.803879
3075.196510	246222.053911	53.808884
3075.273832	246066.726121	53.813889
3074.061743	245929.886981	53.818893
3073.594863	245773.525160	53.823898
3072.920259	245621.525559	53.828903
3072.031818	245473.099695	53.833908
3071.716368	245318.522482	53.838913
3070.837139	245178.142614	53.843917
3070.166496	245026.448633	53.848922
3069.558035	244877.928171	53.853927
3068.815251	244721.203777	53.858932
3068.331302	244569.378899	53.863937
3067.459792	244427.394268	53.868941
3066.715117	244281.722694	53.873946
3066.337922	244133.395645	53.878951
3065.276637	243981.178982	53.883956
3064.964670	243828.894822	53.888961
3063.885057	243691.273034	53.893965
3063.499959	243546.767697	53.898970
3062.969931	243399.458821	53.903975
3061.806680	243251.002548	53.908980
3061.346257	243098.131584	53.913985
3060.823922	242954.259804	53.918989
3060.186108	242812.596466	53.923994
3059.782341	242668.757173	53.928999
3058.913580	242509.508886	53.934004
3058.593373	242355.292445	53.939009
3057.501011	242213.829060	53.944013
3057.065431	242065.437263	53.949018
3056.496684	241916.531960	53.954023
3055.181779	241766.140655	53.959028
3055.237550	241617.085932	53.964033
3054.324260	241472.590202	53.969037
3053.839410	241320.973073	53.974042
3052.802064	241169.087081	53.979047
3052.234066	241025.988724	53.984052
3051.735760	240872.158858	53.989057
3051.075452	240730.730674	53.994061
3050.324924	240573.987214	53.999066
3049.833289	240433.933243	54.004071
3049.006307	240292.531968	54.009076
3048.726882	240132.480522	54.014081
3048.107920	239981.828524	54.019085
3047.402460	239826.555876	54.024090
3046.360065	239674.239719	54.029095
3045.611942	239533.998253	54.034100
3044.993770	239370.869359	54.039105
3044.547173	239230.453214	54.044109
3043.566558	239080.674507	54.049114
3043.126147	238925.870416	54.054119
3042.215172	238792.454612	54.059124
3041.896041	238632.920837	54.064129
3040.901788	238486.251718	54.069133
3040.186218	238338.825683	54.074138
3039.715038	238201.139385	54.079143
3039.220776	238048.178453	54.084148
3038.401010	237892.188110	54.089153
3037.613242	237756.818784	54.094157
3037.106864	237604.013175	54.099162
3035.988276	237454.844182	54.104167
3035.403995	237315.190715	54.109172
3034.667365	237175.230516	54.114177
3034.093634	237037.816561	54.119181
3033.666571	236894.879381	54.124186
3033.217016	236748.966689	54.129191
3032.237535	236593.843813	54.134196
3031.681694	236452.582757	54.139201
3030.856618	236316.024364	54.144205
3030.121657	236166.669131	54.149210
3029.731854	236020.060471	54.154215
3028.998693	235887.460412	54.159220
3028.357897	235731.113877	54.164225
3027.575684	235597.477949	54.169229
3026.806110	235441.559654	54.174234
3026.230306	235302.951521	54.179239
3025.390057	235163.061341	54.184244
3024.895873	235017.616483	54.189249
3024.089263	234877.644980	54.194253
3023.371682	234736.564656	54.199258
3022.857507	234593.160637	54.204263
3022.086971	234450.052037	54.209268
3021.152597	234300.832950	54.214273
3020.313128	234162.955626	54.219277
3020.080367	234015.230078	54.224282
3019.070044	233885.019121	54.229287
3018.701695	233763.746090	54.234292
3018.473279	233608.814420	54.239297
3017.684677	233475.538808	54.244301
3016.919524	233335.002729	54.249306
3016.288059	233184.718863	54.254311
3015.702385	233050.469582	54.259316
3015.245344	232907.848317	54.264321
3014.652540	232753.637725	54.269325
3013.770314	232603.368997	54.274330
3013.124452	232457.340821	54.279335
3012.332406	232319.916929	54.284340
3011.944682	232172.142326	54.289345
3010.891950	232039.725321	54.294349
3010.356725	231884.972304	54.299354
3009.953150	231736.106003	54.304359
3008.988076	231596.495317	54.309364
3008.538243	231457.439833	54.314369
3007.710988	231318.775317	54.319373
3007.439623	231169.303353	54.324378
3006.335666	231023.502698	54.329383
3005.647111	230876.287012	54.334388
3005.381431	230729.513860	54.339393
3004.655006	230588.822962	54.344397
3004.331813	230443.790802	54.349402
3003.537518	230299.189922	54.354407
3002.628946	230152.544936	54.359412
3001.831582	230000.051777	54.364417
3001.319996	229850.365376	54.369421
3000.805196	229713.716251	54.374426
2999.971313	229567.595093	54.379431
2999.103715	229430.493014	54.384436
2998.439687	229268.788255	54.389441
2997.688378	229136.353195	54.394445
2996.876124	228995.169140	54.399450
2996.393260	228839.674613	54.404455
2995.829832	228702.016273	54.409460
2995.237825	228562.453053	54.414465
2994.324428	228426.352787	54.419469
2993.651643	228275.446950	54.424474
2993.245898	228136.873385	54.429479
2992.393033	228003.895961	54.434484
2991.831307	227846.735232	54.439489
2991.280770	227715.950994	54.444493
2990.522405	227567.275081	54.449498
2989.783396	227418.163520	54.454503
2988.904489	227287.635612	54.459508
2988.723875	227141.389637	54.464513
2987.917034	227007.795406	54.469517
2987.284167	226861.137751	54.474522
2986.445526	226716.091515	54.479527
2985.393847	226579.901502	54.484532
2985.085993	226436.210265	54.489537
2984.475830	226294.731315	54.494541
2983.897355	226165.519743	54.499546
2983.324099	226010.197433	54.504551
2982.460108	225875.977534	54.509556
2982.116930	225725.546000	54.514561
2981.164858	225586.668465	54.519565
2980.532816	225442.584710	54.524570
2980.037986	225302.820524	54.529575
2978.964168	225166.356276	54.534580
2978.889200	225016.405522	54.539585
2977.775599	224883.728939	54.544589
2977.074951	224735.634535	54.549594
2976.362875	224596.071451	54.554599
2975.761919	224455.154347	54.559604
2975.365461	224315.796384	54.564609
2974.384237	224170.942711	54.569613
2973.826747	224030.732359	54.574618
2973.184884	223902.845616	54.579623
2972.403688	223761.945539	54.584628
2971.984486	223613.121228	54.589633
2971.425823	223480.982886	54.594637
2970.569725	223331.795455	54.599642
2970.115499	223188.336824	54.604647
2969.194558	223052.030204	54.609652
2968.789234	222910.448374	54.614657
2967.922372	222773.204394	54.619661
2967.258065	222624.127977	54.624666
2966.812106	222476.952216	54.629671
2965.773729	222339.074207	54.634676
2965.198256	222200.435745	54.639681
2964.435946	222063.647475	54.644685
2963.644628	221927.500530	54.649690
2963.521734	221781.140574	54.654695
2962.529544	221656.189909	54.659700
2962.025603	221509.636210	54.664705
2961.286603	221371.457951	54.669709
2960.744856	221230.091758	54.674714
2959.646324	221082.996540	54.679719
2958.934704	220951.064967	54.684724
2958.630708	220804.162737	54.689729
2957.961750	220672.886836	54.694733
2957.163714	220531.918962	54.699738
2956.605963	220402.904516	54.704743
2955.753317	220267.483130	54.709748
2955.175499	220126.824852	54.714753
2954.347898	219994.900603	54.719757
2953.712785	219845.023082	54.724762
2953.680088	219710.796753	54.729767
2952.478961	219574.871718	54.734772
2951.426680	219428.116148	54.739777
2950.859691	219301.841902	54.744781
2950.367543	219168.885867	54.749786
2949.550177	219024.016041	54.754791
2948.598280	218895.308504	54.759796
2948.453731	218766.104219	54.764801
2947.951523	218643.385046	54.769805
2947.388746	218511.383362	54.774810
2946.749740	218361.815012	54.779815
2945.901006	218231.870326	54.784820
2945.370104	218091.132177	54.789825
2944.660202	217953.592192	54.794829
2943.824574	217818.249049	54.799834
2943.217801	217678.873009	54.804839
2942.401829	217552.679443	54.809844
2942.011789	217401.902617	54.814849
2940.762769	217270.928375	54.819853
2940.243426	217145.350478	54.824858
2939.877255	217019.303040	54.829863
2938.885804	216884.737367	54.834868
2938.698958	216750.604626	54.839873
2937.832941	216623.084123	54.844877
2937.426798	216481.667532	54.849882
2936.602775	216343.881459	54.854887
2935.850095	216217.260229	54.859892
2935.067827	216072.085396	54.864897
2934.565029	215940.308151	54.869901
2933.844433	215810.284019	54.874906
2933.472268	215671.383990	54.879911
2932.383832	215540.120288	54.884916
2931.576303	215408.150473	54.889921
2931.187248	215274.141718	54.894925
2930.427148	215138.104491	54.899930
2929.836504	215012.681776	54.904935
2929.017011	214882.547787	54.909940
2928.543762	214744.951235	54.914945
2927.833000	214617.028029	54.919949
2927.502263	214486.308276	54.924954
2926.854801	214343.445092	54.929959
2926.326608	214205.641960	54.934964
2925.598539	214053.754994	54.939969
2924.709067	213928.025224	54.944973
2924.032929	213787.840723	54.949978
2923.507137	213657.089836	54.954983
2922.605461	213536.695897	54.959988
2922.270229	213388.337623	54.964993
2921.380515	213255.481353	54.969997
2920.583571	213120.765073	54.975002
2919.999891	212974.827243	54.980007
2919.297850	212844.436808	54.985012
2918.569583	212706.095715	54.990017
2917.821974	212581.377031	54.995021
2917.226561	212448.844912	55.000026
2916.706427	212311.451762	55.005031
2915.901512	212183.840924	55.010036
2915.593182	212056.253529	55.015041
2914.774361	211924.623361	55.020045
2913.908573	211793.879127	55.025050
2913.295630	211642.755928	55.030055
2912.989477	211522.551431	55.035060
2912.053812	211377.843899	55.040065
2911.390498	211251.599825	55.045069
2911.013622	211110.546398	55.050074
2910.314656	210977.460958	55.055079
2909.060657	210846.360119	55.060084
2908.677438	210704.888582	55.065089
2908.030011	210572.801321	55.070093
2907.031112	210436.111667	55.075098
2906.221805	210312.743579	55.080103
2905.700764	210189.979195	55.085108
2905.262392	210058.674478	55.090113
2904.644584	209924.407473	55.095117
2904.302461	209793.482625	55.100122
2903.852159	209662.066082	55.105127
2902.927407	209525.404860	55.110132
2902.635747	209391.443728	55.115137
2901.604000	209258.160085	55.120141
2900.993483	209122.913645	55.125146
2900.193731	208980.111957	55.130151
2899.170487	208850.289693	55.135156
2898.839496	208723.858095	55.140161
2898.457324	208596.543952	55.145165
2897.426331	208461.543733	55.150170
2897.021594	208323.250109	55.155175
2895.878944	208188.662720	55.160180
2895.169885	208046.536119	55.165185
2894.644033	207917.960701	55.170189
2893.667806	207795.400437	55.175194
2893.368466	207668.724201	55.180199
2892.431354	207541.500144	55.185204
2892.102132	207402.382130	55.190209
2891.249209	207276.863451	55.195213
2890.734514	207143.960733	55.200218
2890.233681	207010.763394	55.205223
2889.214629	206892.284380	55.210228
2888.487143	206761.197979	55.215233
2887.731789	206630.307183	55.220237
2887.375788	206503.553293	55.225242
2886.632214	206381.175440	55.230247
2885.996614	206248.293866	55.235252
2885.395269	206108.687437	55.240257
2884.578114	205986.767489	55.245261
2883.756599	205859.541448	55.250266
2883.472318	205728.285337	55.255271
2882.584055	205605.588387	55.260276
2882.156178	205473.579260	55.265281
2881.579501	205343.681156	55.270285
2880.781422	205217.992715	55.275290
2880.026470	205087.194375	55.280295
2879.355796	204964.222513	55.285300
2878.831465	204830.944738	55.290305
2877.803404	204704.301165	55.295309
2877.174888	204579.579919	55.300314
2876.925805	204450.230079	55.305319
2876.170258	204325.389509	55.310324
2875.714275	204198.363746	55.315329
2874.976108	204062.258184	55.320333
2874.213130	203929.249361	55.325338
2873.404843	203798.398760	55.330343
2872.558283	203674.732111	55.335348
2872.375539	203540.868732	55.340353
2871.756797	203418.948229	55.345357
2871.022600	203285.020068	55.350362
2870.482664	203145.334711	55.355367
2869.479277	203015.916681	55.360372
2868.885183	202879.256639	55.365377
2868.169878	202765.662945	55.370381
2867.293629	202623.677826	55.375386
2866.930806	202504.225789	55.380391
2866.403161	202376.057391	55.385396
2865.676583	202239.419887	55.390401
2864.871278	202109.158121	55.395405
2864.048899	201976.545082	55.400410
2863.407198	201856.858625	55.405415
2862.559113	201734.354533	55.410420
2862.285637	201605.638624	55.415425
2861.534107	201476.107920	55.420429
2860.924249	201343.322757	55.425434
2860.242608	201213.921582	55.430439
2859.502092	201097.204773	55.435444
2859.570546	200959.770057	55.440449
2858.459905	200827.396312	55.445453
2857.518199	200696.879514	55.450458
2856.844075	200568.038596	55.455463
2856.275223	200442.159075	55.460468
2855.367165	200305.847787	55.465473
2854.881091	200181.890027	55.470477
2853.998590	200055.170293	55.475482
2853.710794	199928.114891	55.480487
2852.459992	199803.706464	55.485492
2852.175654	199676.434774	55.490497
2851.636889	199553.301217	55.495501
2850.815806	199420.745067	55.500506
2850.294762	199294.606137	55.505511
2849.301723	199171.087293	55.510516
2848.858506	199052.482644	55.515521
2848.214791	198922.800972	55.520525
2847.253076	198800.143332	55.525530
2846.891765	198677.874439	55.530535
2845.890243	198555.961721	55.535540
2845.507344	198430.032004	55.540545
2844.724653	198315.262089	55.545549
2843.859667	198192.221509	55.550554
2843.518485	198061.425128	55.555559
2842.797579	197938.985840	55.560564
2842.266787	197813.246437	55.565569
2841.606037	197691.243568	55.570573
2840.975751	197570.126894	55.575578
2840.433435	197433.637763	55.580583
2839.414236	197315.382723	55.585588
2838.892958	197179.641682	55.590593
2838.324268	197052.395864	55.595597
2837.486647	196937.510412	55.600602
2837.016067	196801.482384	55.605607
2836.039473	196687.077581	55.610612
2835.298415	196556.984518	55.615617
2834.909142	196445.159388	55.620621
2834.355266	196311.805264	55.625626
2833.871880	196192.691723	55.630631
2832.708075	196067.845704	55.635636
2832.441663	195947.362301	55.640641
2831.906201	195816.856808	55.645645
2831.041464	195697.970229	55.650650
2830.515714	195556.520922	55.655655
2829.802198	195429.276592	55.660660
2829.083366	195302.567840	55.665665
2828.503651	195180.812538	55.670669
2827.786260	195060.084544	55.675674
2827.234493	194924.214306	55.680679
2826.295721	194792.757377	55.685684
2825.889925	194655.846809	55.690689
2825.284435	194543.067602	55.695693
2824.289388	194415.374164	55.700698
2823.676398	194287.633262	55.705703
2823.007228	194160.359645	55.710708
2822.443241	194037.395828	55.715713
2821.343249	193916.362171	55.720717
2820.540003	193799.111693	55.725722
2820.403899	193659.959890	55.730727
2819.725445	193545.527657	55.735732
2819.250757	193417.092707	55.740737
2818.462914	193301.609562	55.745741
2817.478086	193174.821057	55.750746
2817.026843	193054.144795	55.755751
2816.376692	192931.973494	55.760756
2816.163598	192794.732126	55.765761
2814.897784	192677.341256	55.770765
2814.491801	192554.572377	55.775770
2813.685635	192428.648136	55.780775
2813.059368	192309.820877	55.785780
2812.356363	192183.740965	55.790785
2811.755199	192062.632830	55.795789
2810.862740	191940.820452	55.800794
2810.459148	191805.673204	55.805799
2809.786208	191685.480730	55.810804
2809.131029	191561.583259	55.815809
2808.454551	191439.865155	55.820813
2807.951216	191322.929314	55.825818
2807.658585	191191.481378	55.830823
2806.652100	191071.305082	55.835828
2805.573964	190942.450533	55.840833
2805.436808	190814.337902	55.845837
2804.699018	190687.109576	55.850842
2803.971377	190567.081215	55.855847
2803.268353	190433.588320	55.860852
2802.501021	190301.607291	55.865857
2801.786607	190187.264949	55.870861
2800.924086	190065.974189	55.875866
2800.548676	189938.970351	55.880871
2799.683360	189820.047111	55.885876
2799.063057	189696.059853	55.890881
2798.301592	189579.054631	55.895885
2797.974758	189453.074937	55.900890
2797.273733	189325.386391	55.905895
2796.116926	189211.778043	55.910900
2795.836772	189079.659619	55.915905
2794.906121	188963.853196	55.920909
2794.322025	188840.218673	55.925914
2793.943443	188715.546840	55.930919
2793.280944	188603.502869	55.935924
2792.765916	188466.766924	55.940929
2792.056261	188352.199249	55.945933
2791.680930	188232.019206	55.950938
2790.579586	188102.794358	55.955943
2789.645199	187982.678062	55.960948
2789.084918	187845.569430	55.965953
2788.643817	187734.777421	55.970957
2787.664111	187612.506472	55.975962
2787.575285	187486.443458	55.980967
2786.256801	187366.542260	55.985972
2785.858009	187239.307686	55.990977
2785.285520	187130.128199	55.995981
2784.564375	187002.945335	56.000986
2784.125782	186869.573322	56.005991
2783.145030	186753.958433	56.010996
2782.691026	186622.001720	56.016001
2782.208744	186501.550492	56.021005
2781.067169	186380.122650	56.026010
2781.043088	186256.279071	56.031015
2780.143531	186131.773026	56.036020
2779.355130	186007.491427	56.041025
2778.474799	185885.845413	56.046029
2777.774326	185752.479965	56.051034
2777.280685	185633.597595	56.056039
2776.224240	185529.943463	56.061044
2775.751674	185392.930016	56.066049
2775.293218	185270.900780	56.071053
2774.574614	185164.407942	56.076058
2773.949604	185035.218042	56.081063
2773.448157	184915.651829	56.086068
2772.927685	184786.675069	56.091073
2772.074603	184673.335106	56.096077
2771.356237	184543.945138	56.101082
2770.803278	184423.459731	56.106087
2769.913346	184303.918518	56.111092
2769.567470	184172.447928	56.116097
2768.945840	184050.714994	56.121101
2767.705129	183930.492512	56.126106
2767.616410	183803.053062	56.131111
2766.687039	183691.902991	56.136116
2766.050600	183564.423774	56.141121
2765.612466	183443.630236	56.146125
2764.863205	183320.367546	56.151130
2764.321877	183186.068594	56.156135
2763.042996	183066.083479	56.161140
2762.781650	182940.709203	56.166145
2762.156448	182821.308136	56.171149
2761.183049	182705.473507	56.176154
2760.853109	182572.465906	56.181159
2760.122141	182454.125697	56.186164
2759.512262	182332.840852	56.191169
2758.643115	182209.511215	56.196173
2758.114906	182094.867027	56.201178
2757.552579	181970.497247	56.206183
2756.645589	181861.905100	56.211188
2756.270131	181727.686094	56.216193
2755.686440	181604.987137	56.221197
2754.885716	181478.939251	56.226202
2754.250076	181357.241421	56.231207
2753.719540	181236.125143	56.236212
2753.197721	181103.686670	56.241217
2752.438587	180991.740533	56.246221
2751.534352	180857.722465	56.251226
2751.129568	180724.719640	56.256231
2750.118705	180608.120591	56.261236
2749.707854	180481.810328	56.266241
2749.238183	180357.506821	56.271245
2748.177467	180234.989082	56.276250
2747.474172	180109.934653	56.281255
2746.868017	179992.509961	56.286260
2746.251765	179858.423951	56.291265
2745.890215	179734.524885	56.296269
2744.907385	179614.375226	56.301274
2744.339106	179485.332612	56.306279
2743.478655	179375.314736	56.311284
2742.789192	179243.760796	56.316289
2742.183861	179119.482385	56.321293
2741.505841	179003.191150	56.326298
2740.934768	178874.646907	56.331303
2740.006486	178749.619400	56.336308
2739.509153	178632.193949	56.341313
2738.758250	178521.067050	56.346317
2738.180388	178397.816700	56.351322
2737.681373	178271.043625	56.356327
2736.776120	178157.538144	56.361332
2736.244381	178028.341558	56.366337
2735.524625	177908.282275	56.371341
2735.123186	177789.101425	56.376346
2734.650700	177667.273823	56.381351
2733.711310	177552.885035	56.386356
2733.120948	177419.158818	56.391361
2732.600025	177298.039528	56.396365
2731.862347	177171.956277	56.401370
2731.171943	177038.170818	56.406375
2730.230779	176916.483258	56.411380
2729.542122	176796.358660	56.416385
2729.014395	176678.053181	56.421389
2728.404401	176552.803765	56.426394
2727.993289	176429.520103	56.431399
2727.037416	176305.089373	56.436404
2726.464217	176169.850917	56.441409
2725.791248	176061.707188	56.446413
2724.650774	175941.911037	56.451418
2724.158151	175807.424140	56.456423
2723.726081	175690.225601	56.461428
2723.066530	175574.309871	56.466433
2722.151973	175457.519124	56.471437
2721.612809	175323.384596	56.476442
2721.272796	175203.323894	56.481447
2720.275362	175088.684061	56.486452
2719.794816	174962.872100	56.491457
2719.369222	174839.646396	56.496461
2718.371744	174722.591091	56.501466
2717.900242	174591.233602	56.506471
2717.136621	174477.652239	56.511476
2716.509017	174347.223280	56.516481
2715.934916	174227.215272	56.521485
2714.973688	174111.669472	56.526490
2714.535000	173985.128981	56.531495
2713.923280	173860.104328	56.536500
2713.843330	173734.525246	56.541505
2712.806305	173611.667241	56.546509
2711.752940	173489.142873	56.551514
2711.242464	173358.609539	56.556519
2710.602631	173229.839489	56.561524
2710.198046	173109.299250	56.566529
2709.654918	172985.016823	56.571533
2708.562318	172856.192533	56.576538
2708.170740	172724.726751	56.581543
2707.312032	172606.193092	56.586548
2706.953895	172474.188693	56.591553
2706.109793	172349.828760	56.596557
2705.415244	172225.687160	56.601562
2704.795651	172093.242184	56.606567
2704.000970	171976.099208	56.611572
2703.336999	171836.972674	56.616577
2703.020926	171720.199746	56.621581
2702.217820	171597.043855	56.626586
2701.505395	171459.299819	56.631591
2700.816125	171340.984751	56.636596
2700.076761	171203.347622	56.641601
2699.551361	171079.844142	56.646605
2698.744989	170952.901040	56.651610
2698.552216	170822.872591	56.656615
2697.542756	170701.049370	56.661620
2697.053995	170575.303460	56.666625
2696.169000	170452.863592	56.671629
2695.607474	170320.847791	56.676634
2695.136213	170187.393834	56.681639
2694.172772	170069.812783	56.686644
2693.705357	169931.793706	56.691649
2693.210153	169800.799241	56.696653
2692.715801	169676.036334	56.701658
2691.982697	169539.014518	56.706663
2691.094370	169409.151879	56.711668
2690.485915	169261.200335	56.716673
2689.446596	169144.626032	56.721677
2689.155614	169011.198448	56.726682
2688.455136	168889.929670	56.731687
2687.931078	168761.969860	56.736692
2687.099758	168632.227986	56.741697
2686.293226	168499.392529	56.746701
2685.657581	168385.159993	56.751706
2685.564949	168241.263500	56.756711
2684.199325	168111.112117	56.761716
2683.547774	167989.050041	56.766721
2682.966067	167856.384669	56.771725
2682.203593	167725.744844	56.776730
2681.952384	167592.850003	56.781735
2680.863584	167473.681850	56.786740
2680.135651	167345.225037	56.791745
2679.614347	167220.042086	56.796749
2679.003870	167092.788261	56.801754
2678.159296	166966.309481	56.806759
2677.484544	166848.756206	56.811764
2676.752792	166715.470109	56.816769
2676.164222	166592.003832	56.821773
2675.516945	166471.675340	56.826778
2675.485195	166335.151608	56.831783
2674.697888	166213.396543	56.836788
2674.310236	166075.544140	56.841793
2673.403991	165940.457402	56.846797
2672.578938	165813.903133	56.851802
2672.069918	165679.555483	56.856807
2671.109482	165553.316009	56.861812
2671.006645	165423.660507	56.866817
2670.072793	165284.715045	56.871821
2669.069686	165163.023046	56.876826
2668.699087	165027.549595	56.881831
2667.744420	164898.247062	56.886836
2667.397502	164755.713906	56.891841
2666.684048	164621.733085	56.896845
2665.803504	164500.405307	56.901850
2665.077242	164363.922582	56.906855
2664.216341	164241.664350	56.911860
2663.807862	164105.361105	56.916865
2663.191476	163986.561594	56.921869
2662.739815	163861.200925	56.926874
2662.248521	163724.492630	56.931879
2661.280829	163598.718749	56.936884
2660.549110	163464.910347	56.941889
2660.383201	163326.244778	56.946893
2659.462748	163196.561395	56.951898
2658.771795	163056.746728	56.956903
2657.690220	162935.087286	56.961908
2657.325030	162794.611715	56.966913
2656.783584	162677.559204	56.971917
2655.864683	162544.940870	56.976922
2655.642084	162408.258528	56.981927
2654.640441	162277.014726	56.986932
2653.904524	162147.750867	56.991937
2653.597344	162018.355967	56.996941
2653.060507	161883.073116	57.001946
2652.433944	161745.961445	57.006951
2651.421341	161616.959478	57.011956
2650.993331	161477.757691	57.016961
2650.355848	161344.056648	57.021965
2649.435597	161219.821939	57.026970
2649.214091	161075.872125	57.031975
2648.169400	160952.942167	57.036980
2647.568343	160807.286355	57.041985
2647.057171	160674.495916	57.046989
2646.444983	160531.309465	57.051994
2645.400867	160401.910055	57.056999
2644.973544	160269.845237	57.062004
2644.193944	160133.590405	57.067009
2643.587361	159994.460860	57.072013
2642.551319	159868.520195	57.077018
2642.479851	159729.599311	57.082023
2641.698061	159609.213184	57.087028
2640.890364	159470.473549	57.092033
2640.204385	159343.958047	57.097037
2639.629311	159207.216713	57.102042
2639.219727	159068.974962	57.107047
2638.167261	158944.807343	57.112052
2637.545184	158795.387374	57.117057
2637.033542	158675.902413	57.122061
2636.281648	158548.472181	57.127066
2635.790715	158417.657562	57.132071
2635.106921	158280.987932	57.137076
2634.339713	158141.713215	57.142081
2633.758924	158005.536859	57.147085
2632.908978	157862.640518	57.152090
2632.021299	157739.353693	57.157095
2631.459356	157615.341921	57.162100
2630.920103	157468.228231	57.167105
2630.278516	157337.784798	57.172109
2629.630455	157207.762396	57.177114
2629.196300	157064.854317	57.182119
2628.504041	156933.555998	57.187124
2627.907598	156806.743164	57.192129
2627.335452	156680.689686	57.197133
2626.690400	156540.499499	57.202138
2626.251933	156399.133052	57.207143
2625.466659	156264.152789	57.212148
2624.838529	156112.113966	57.217153
2624.249552	155973.391819	57.222157
2623.359310	155837.806986	57.227162
2622.527575	155691.853203	57.232167
2621.872628	155556.677121	57.237172
2621.245747	155416.552231	57.242177
2620.636930	155277.238611	57.247181
2620.125491	155145.041404	57.252186
2619.512635	155006.848166	57.257191
2618.475967	154877.163166	57.262196
2618.248466	154731.766057	57.267201
2617.361790	154588.342624	57.272205
2616.566506	154452.341521	57.277210
2616.235509	154303.479720	57.282215
2615.516289	154164.315299	57.287220
2614.586604	154026.608473	57.292225
2614.035170	153899.329050	57.297229
2613.252728	153766.442945	57.302234
2612.871564	153619.104761	57.307239
2611.890808	153486.810485	57.312244
2611.345952	153338.940188	57.317249
2610.796114	153205.511012	57.322253
2610.005108	153070.607986	57.327258
2609.624733	152931.483977	57.332263
2608.650914	152800.614945	57.337268
2608.085640	152646.141329	57.342273
2607.758715	152514.319291	57.347277
2606.912603	152380.927665	57.352282
2606.311236	152227.313336	57.357287
2605.334703	152094.337564	57.362292
2604.774176	151962.122586	57.367297
2603.956542	151815.039518	57.372301
2603.099241	151677.356377	57.377306
2602.715810	151541.022275	57.382311
2602.107522	151411.702324	57.387316
2601.793568	151268.393100	57.392321
2601.068131	151134.402728	57.397325
2600.069202	150990.351688	57.402330
2599.570072	150854.674280	57.407335
2598.951531	150645.133048	57.412340
2598.325263	150503.020569	57.417345
2597.857716	150363.323854	57.422349
2597.011777	150229.152935	57.427354
2596.355900	150078.709348	57.432359
2595.284336	149950.243898	57.437364
2594.545764	149803.665739	57.442369
2593.982510	149661.267341	57.447373
2593.477732	149529.180466	57.452378
2593.366157	149392.278459	57.457383
2592.263308	149261.177126	57.462388
2591.356997	149115.251433	57.467393
2590.964917	148978.942137	57.472397
2590.179505	148843.280380	57.477402
2589.549590	148701.761012	57.482407
2588.997764	148555.857933	57.487412
2588.462098	148432.422692	57.492417
2587.890938	148280.766693	57.497421
2587.198577	148139.361374	57.502426
2586.374760	147990.568192	57.507431
2585.549863	147847.177157	57.512436
2585.012512	147715.052065	57.517441
2584.487143	147564.777471	57.522445
2583.580223	147424.248105	57.527450
2583.150399	147285.079830	57.532455
2582.147041	147148.595617	57.537460
2581.821516	147014.152315	57.542465
2581.055527	146872.942210	57.547469
2580.490237	146731.230714	57.552474
2579.783967	146586.555723	57.557479
2579.439766	146452.880268	57.562484
2578.781262	146299.061728	57.567489
2578.078610	146144.539275	57.572493
2577.329380	146013.026730	57.577498
2576.570553	145862.263475	57.582503
2575.955181	145730.120910	57.587508
2575.606055	145578.264735	57.592513
2575.215850	145426.059983	57.597517
2573.700954	145292.371671	57.602522
2573.593371	145128.813569	57.607527
2572.647974	145001.021624	57.612532
2571.841493	144846.776179	57.617537
2571.379011	144704.587350	57.622541
2570.664967	144552.374641	57.627546
2569.967132	144410.033844	57.632551
2569.216620	144261.767668	57.637556
2568.403711	144122.305605	57.642561
2568.083863	143985.587055	57.647565
2567.486967	143844.922930	57.652570
2567.056677	143686.531883	57.657575
2566.195808	143544.030296	57.662580
2565.865710	143401.572317	57.667585
2565.118985	143253.869484	57.672589
2564.434242	143094.873743	57.677594
2563.710940	142955.504405	57.682599
2562.911193	142801.166435	57.687604
2562.164282	142655.652085	57.692609
2561.815450	142502.171749	57.697613
2560.905082	142358.374713	57.702618
2560.173515	142199.645168	57.707623
2559.591622	142056.966497	57.712628
2558.917214	141903.642419	57.717633
2558.116494	141754.583074	57.722637
2557.490503	141609.270554	57.727642
2556.995329	141461.638155	57.732647
2556.068879	141325.993275	57.737652
2555.796608	141169.191186	57.742657
2555.127985	141022.782793	57.747661
2554.380724	140862.855631	57.752666
2553.684944	140715.677959	57.757671
2552.843941	140585.156075	57.762676
2552.366066	140427.615354	57.767681
2551.767498	140276.472895	57.772685
2551.101230	140132.164904	57.777690
2550.617854	139988.603663	57.782695
2549.499312	139826.187009	57.787700
2549.053056	139684.590708	57.792705
2548.417427	139532.682826	57.797709
2547.398132	139393.262426	57.802714
2546.778849	139244.135906	57.807719
2546.233048	139096.942395	57.812724
2545.563664	138954.902111	57.817729
2545.059652	138797.590086	57.822733
2544.258224	138657.261938	57.827738
2543.766531	138506.950013	57.832743
2543.057194	138366.646756	57.837748
2542.171218	138214.899613	57.842753
2541.804612	138058.420951	57.847757
2541.186321	137922.856980	57.852762
2540.476673	137766.154729	57.857767
2539.674410	137627.140177	57.862772
2538.919016	137465.301383	57.867777
2538.111766	137321.969497	57.872781
2537.526346	137180.432593	57.877786
2537.275146	137028.705274	57.882791
2536.389381	136874.830648	57.887796
2535.604385	136737.227745	57.892801
2535.172624	136585.023165	57.897805
2534.306509	136440.193111	57.902810
2533.561347	136283.555206	57.907815
2533.380350	136141.857578	57.912820
2532.750036	135988.290131	57.917825
2532.003298	135846.569272	57.922829
2531.285354	135698.772106	57.927834
2530.867296	135524.580552	57.932839
2530.083555	135373.873601	57.937844
2529.119861	135223.030809	57.942849
2528.571062	135064.246833	57.947853
2527.707729	134933.423156	57.952858
2527.171875	134775.057928	57.957863
2526.500130	134630.510960	57.962868
2526.064828	134486.232117	57.967873
2525.730846	134322.959301	57.972877
2524.709978	134173.083793	57.977882
2524.226891	134020.506986	57.982887
2523.190282	133870.102022	57.987892
2522.468406	133723.966967	57.992897
2522.028656	133561.426604	57.997901
2521.495690	133409.991504	58.002906
2520.969767	133259.775553	58.007911
2519.815032	133108.834388	58.012916
2519.329782	132956.441424	58.017921
2518.860247	132817.778250	58.022925
2517.815548	132662.185571	58.027930
2517.641547	132499.304264	58.032935
2516.731988	132354.184051	58.037940
2515.879952	132208.255218	58.042945
2515.311795	132052.628445	58.047949
2514.206912	131907.566882	58.052954
2513.898734	131749.677686	58.057959
2513.361580	131600.894907	58.062964
2512.967690	131450.883515	58.067969
2512.545032	131306.301186	58.072973
2511.689229	131157.368022	58.077978
2511.074220	130989.560782	58.082983
2510.110880	130838.423545	58.087988
2509.421131	130681.273999	58.092993
2508.765590	130526.101349	58.097997
2508.018207	130378.717413	58.103002
2507.363726	130220.701156	58.108007
2506.281992	130072.584344	58.113012
2505.970420	129924.879689	58.118017
2505.334118	129766.863114	58.123021
2504.785122	129634.210444	58.128026
2504.077777	129480.626746	58.133031
2503.288858	129332.416644	58.138036
2502.770904	129181.522588	58.143041
2501.927693	129033.640208	58.148045
2501.385805	128890.245035	58.153050
2501.118822	128730.054772	58.158055
2500.336995	128585.518041	58.163060
2499.661228	128423.540054	58.168065
2498.958135	128280.453004	58.173069
2497.868393	128120.193484	58.178074
2497.507990	127963.946902	58.183079
2496.998927	127806.505542	58.188084
2496.268527	127674.792728	58.193089
2495.810814	127520.875527	58.198093
2494.949590	127362.832122	58.203098
2494.399777	127202.098658	58.208103
2493.778920	127049.556162	58.213108
2493.166512	126897.978367	58.218113
2492.628491	126743.786159	58.223117
2491.363328	126594.828080	58.228122
2491.320378	126417.369531	58.233127
2490.534372	126269.886628	58.238132
2490.102241	126120.405401	58.243137
2489.347453	125958.784679	58.248141
2488.392021	125805.324318	58.253146
2487.639193	125642.003456	58.258151
2487.017065	125497.698985	58.263156
2486.451887	125335.289965	58.268161
2485.960677	125177.149781	58.273165
2484.961885	125023.129266	58.278170
2484.749959	124876.540756	58.283175
2483.878354	124721.219209	58.288180
2483.116589	124558.350767	58.293185
2482.557696	124398.333756	58.298189
2482.025441	124246.745365	58.303194
2481.272302	124085.211777	58.308199
2480.582846	123933.523088	58.313204
2479.898657	123773.859820	58.318209
2479.677455	123603.190843	58.323213
2478.440867	123459.934375	58.328218
2478.230522	123299.716284	58.333223
2477.690514	123149.900374	58.338228
2476.746257	122979.032553	58.343233
2475.998357	122825.251544	58.348237
2475.138574	122662.753016	58.353242
2474.615278	122493.269137	58.358247
2473.680432	122345.704368	58.363252
2473.126598	122192.480352	58.368257
2472.718934	122038.561076	58.373261
2471.372076	121888.004055	58.378266
2470.865335	121719.106586	58.383271
2470.367498	121574.244879	58.388276
2469.964291	121427.972262	58.393281
2469.366836	121265.199474	58.398285
2468.735239	121117.263361	58.403290
2468.254383	120954.194673	58.408295
2467.198071	120799.382386	58.413300
2466.786388	120630.324460	58.418305
2466.164014	120482.822151	58.423309
2465.504090	120314.046857	58.428314
2464.717493	120164.604377	58.433319
2464.104859	119999.861157	58.438324
2463.420705	119837.174453	58.443329
2462.717236	119688.749935	58.448333
2461.955459	119531.124285	58.453338
2461.528185	119371.338974	58.458343
2460.767894	119216.476437	58.463348
2460.143046	119059.016034	58.468353
2459.543616	118889.313551	58.473357
2458.669245	118739.106009	58.478362
2458.137008	118576.415803	58.483367
2457.253062	118430.724963	58.488372
2456.813859	118268.409166	58.493377
2455.664065	118106.568869	58.498381
2455.139782	117954.361598	58.503386
2454.908172	117795.811846	58.508391
2453.926690	117642.237959	58.513396
2453.341136	117496.587611	58.518401
2453.038745	117335.233542	58.523405
2452.237942	117184.312454	58.528410
2451.535177	117016.796856	58.533415
2450.877966	116854.676876	58.538420
2450.378860	116698.124996	58.543425
2449.700824	116545.683852	58.548429
2448.908971	116391.243185	58.553434
2448.380683	116221.394674	58.558439
2447.729607	116071.268880	58.563444
2447.097005	115905.037954	58.568449
2446.457393	115733.801243	58.573453
2445.705782	115575.322291	58.578458
2444.957637	115412.851408	58.583463
2444.560174	115246.149557	58.588468
2443.913587	115088.006090	58.593473
2442.847643	114921.240987	58.598477
2442.234672	114765.950376	58.603482
2441.617654	114604.917353	58.608487
2440.554899	114454.612520	58.613492
2440.120943	114296.960742	58.618497
2439.742902	114124.620823	58.623501
2438.810967	113976.830493	58.628506
2438.218666	113815.265467	58.633511
2437.603767	113657.310004	58.638516
2436.957376	113503.308170	58.643521
2436.696723	113341.319159	58.648525
2435.592990	113186.896740	58.653530
2435.125308	113014.730972	58.658535
2434.724460	112855.718484	58.663540
2433.787577	112698.607090	58.668545
2433.508499	112532.037733	58.673549
2432.404226	112376.604983	58.678554
2431.617315	112202.984984	58.683559
2431.179216	112050.418750	58.688564
2430.705856	111888.136541	58.693569
2429.957465	111726.819202	58.698573
2428.674657	111574.364436	58.703578
2428.564704	111391.015605	58.708583
2427.512078	111246.801748	58.713588
2427.008723	111083.729953	58.718593
2426.478585	110926.857209	58.723597
2426.066739	110770.182472	58.728602
2425.072658	110607.318549	58.733607
2424.455532	110441.597394	58.738612
2424.087231	110288.351954	58.743617
2423.405266	110110.852685	58.748621
2422.521786	109964.868072	58.753626
2422.145488	109791.866230	58.758631
2421.155069	109645.386471	58.763636
2420.467800	109473.451495	58.768641
2419.800267	109311.629510	58.773645
2419.106586	109146.297295	58.778650
2418.322900	109001.692290	58.783655
2417.950855	108834.775570	58.788660
2417.360566	108682.216279	58.793665
2416.900103	108516.743485	58.798669
2416.139928	108360.919878	58.803674
2415.728847	108181.272334	58.808679
2414.816112	108023.444580	58.813684
2414.151023	107851.720590	58.818689
2413.587188	107677.240642	58.823693
2412.767269	107526.958532	58.828698
2412.189756	107343.834720	58.833703
2411.739211	107192.125586	58.838708
2410.913171	107025.509038	58.843713
2410.153011	106854.099087	58.848717
2409.327026	106695.542932	58.853722
2408.624087	106529.963557	58.858727
2408.258592	106366.305066	58.863732
2407.181311	106207.849080	58.868737
2406.891791	106035.348836	58.873741
2405.930974	105874.846265	58.878746
2405.216505	105708.018143	58.883751
2404.470432	105550.326114	58.888756
2403.608607	105387.381130	58.893761
2403.557238	105239.725998	58.898765
2402.761161	105070.307664	58.903770
2402.324120	104896.950801	58.908775
2401.409632	104748.820154	58.913780
2400.872714	104573.038889	58.918785
2400.395360	104418.896316	58.923789
2399.620173	104255.989757	58.928794
2399.193389	104081.488906	58.933799
2398.108714	103922.491011	58.938804
2397.381465	103748.852312	58.943809
2397.305299	103585.027485	58.948813
2396.241189	103424.272367	58.953818
2395.779585	103260.675853	58.958823
2394.902727	103095.611077	58.963828
2394.372410	102926.755937	58.968833
2393.650406	102747.084371	58.973837
2392.610080	102582.220405	58.978842
2392.324695	102427.901806	58.983847
2391.516717	102260.389620	58.988852
2391.230644	102102.742803	58.993857
2390.573240	101927.723553	58.998861
2389.398824	101758.572966	59.003866
2388.984415	101594.764905	59.008871
2388.412975	101440.764605	59.013876
2387.310043	101272.709982	59.018881
2386.675809	101110.120071	59.023885
2386.022514	100952.666122	59.028890
2385.833264	100772.087942	59.033895
2384.953203	100634.495059	59.038900
2383.967683	100459.209025	59.043905
2383.463583	100295.088150	59.048909
2382.853858	100130.395271	59.053914
2382.152056	99970.228126	59.058919
2381.436318	99811.808647	59.063924
2381.053014	99640.917882	59.068929
2380.726839	99477.212270	59.073933
2379.661806	99317.468804	59.078938
2379.162970	99148.528264	59.083943
2378.386877	98974.723565	59.088948
2377.820297	98809.697110	59.093953
2377.041397	98647.033301	59.098957
2376.200682	98481.798965	59.103962
2375.502712	98314.640385	59.108967
2374.919658	98153.350757	59.113972
2374.305261	97989.561919	59.118977
2373.636819	97822.053417	59.123981
2372.877413	97676.765614	59.128986
2372.673401	97507.980700	59.133991
2371.721065	97344.446697	59.138996
2371.497924	97181.527610	59.144001
2370.691371	97005.840010	59.149005
2369.912174	96848.078989	59.154010
2369.424748	96670.047485	59.159015
2368.358663	96505.808206	59.164020
2367.509846	96337.952371	59.169025
2367.113999	96177.401779	59.174029
2366.329906	96014.599053	59.179034
2365.768355	95836.427311	59.184039
2365.275061	95689.188425	59.189044
2364.547237	95521.757063	59.194049
2363.900402	95355.969324	59.199053
2362.913721	95193.972014	59.204058
2362.753109	95015.705133	59.209063
2361.786151	94858.831242	59.214068
2361.259490	94688.444323	59.219073
2360.890157	94526.499792	59.224077
2359.749765	94356.250772	59.229082
2359.398972	94180.595359	59.234087
2358.730638	94016.812162	59.239092
2357.848709	93857.376200	59.244097
2357.480872	93688.810719	59.249101
2356.827338	93518.243572	59.254106
2356.219547	93343.979857	59.259111
2355.516379	93182.396053	59.264116
2354.762534	93005.754827	59.269121
2354.005767	92832.298713	59.274125
2353.463907	92673.755794	59.279130
2352.596469	92507.421781	59.284135
2351.985095	92334.250878	59.289140
2351.048589	92168.241077	59.294145
2350.616985	91996.990974	59.299149
2349.786256	91843.173049	59.304154
2349.130524	91666.634746	59.309159
2348.614981	91501.368485	59.314164
2347.918937	91337.812372	59.319169
2347.324755	91166.125293	59.324173
2346.716134	91015.695535	59.329178
2346.117663	90844.892991	59.334183
2345.503152	90672.160466	59.339188
2344.781330	90515.830057	59.344193
2344.249475	90332.828240	59.349197
2343.410851	90172.302440	59.354202
2342.786207	89998.701866	59.359207
2341.792662	89839.889599	59.364212
2341.135014	89662.581539	59.369217
2340.852153	89494.060010	59.374221
2340.031119	89338.159537	59.379226
2339.534731	89152.061680	59.384231
2338.924834	89011.130660	59.389236
2338.090027	88838.010128	59.394241
2337.526084	88656.200373	59.399245
2336.784521	88495.500370	59.404250
2336.438250	88316.873256	59.409255
2335.786550	88157.467514	59.414260
2334.833113	87980.461012	59.419265
2334.165693	87815.525711	59.424269
2333.250715	87655.233497	59.429274
2332.852469	87476.038332	59.434279
2332.214188	87311.951765	59.439284
2331.256908	87155.182078	59.444289
2330.634462	86983.982610	59.449293
2330.098452	86813.011695	59.454298
2329.770492	86646.034618	59.459303
2328.973653	86489.206315	59.464308
2328.271150	86312.516067	59.469313
2328.049794	86147.693983	59.474317
2327.103689	85985.916785	59.479322
2326.198746	85798.638507	59.484327
2325.703329	85638.034929	59.489332
2324.855702	85463.878631	59.494337
2324.490860	85294.718331	59.499341
2323.375009	85146.558748	59.504346
2322.770704	84956.064417	59.509351
2322.276378	84788.836662	59.514356
2321.602459	84628.871194	59.519361
2321.164542	84448.642785	59.524365
2320.310001	84293.760414	59.529370
2319.643987	84120.587833	59.534375
2319.157179	83946.988921	59.539380
2318.435926	83776.318960	59.544385
2317.879750	83597.897664	59.549389
2317.365280	83437.491243	59.554394
2316.677150	83259.752925	59.559399
2315.869776	83090.300118	59.564404
2315.140419	82913.205092	59.569409
2314.786100	82743.771959	59.574413
2313.951277	82572.831871	59.579418
2313.214188	82394.354401	59.584423
2312.456487	82225.255628	59.589428
2311.916526	82053.544141	59.594433
2311.339651	81881.554711	59.599437
2310.363378	81704.490045	59.604442
2310.014113	81535.547559	59.609447
2309.376657	81358.552510	59.614452
2308.547274	81196.920278	59.619457
2308.012174	81009.131549	59.624461
2307.046888	80851.066297	59.629466
2306.491570	80668.315897	59.634471
2305.976307	80490.459622	59.639476
2305.124912	80334.737780	59.644481
2304.725360	80155.826683	59.649485
2303.609783	79991.308684	59.654490
2303.342097	79808.095645	59.659495
2302.671765	79641.627642	59.664500
2302.090339	79486.604482	59.669505
2301.169312	79305.901305	59.674509
2300.695493	79130.870161	59.679514
2300.008316	78958.098632	59.684519
2299.250272	78782.164978	59.689524
2298.597392	78612.400966	59.694529
2298.208996	78444.731927	59.699533
2297.364714	78280.197236	59.704538
2296.734148	78098.501744	59.709543
2296.199982	77923.756593	59.714548
2295.246690	77756.417235	59.719553
2294.850636	77571.020314	59.724557
2293.809365	77405.852217	59.729562
2293.222441	77240.499339	59.734567
2292.766391	77066.705934	59.739572
2291.760923	76883.540952	59.744577
2291.312302	76710.991329	59.749581
2290.358708	76546.671694	59.754586
2290.109699	76368.320984	59.759591
2289.526471	76217.384368	59.764596
2288.673523	76033.607256	59.769601
2288.307296	75861.761421	59.774605
2287.396469	75695.129241	59.779610
2286.892008	75519.164496	59.784615
2285.887977	75345.770522	59.789620
2285.540688	75180.839919	59.794625
2284.875588	74991.004433	59.799629
2284.065569	74827.791075	59.804634
2283.390362	74650.783907	59.809639
2282.869070	74486.615182	59.814644
2282.305165	74317.075661	59.819649
2281.767038	74139.081911	59.824653
2280.822825	73963.796032	59.829658
2280.155641	73799.643390	59.834663
2279.683394	73616.138367	59.839668
2278.877110	73449.197766	59.844673
2278.226269	73260.301324	59.849677
2277.285167	73101.576464	59.854682
2276.639742	72912.606427	59.859687
2275.900043	72749.715587	59.864692
2275.065821	72583.312467	59.869697
2274.861224	72405.800708	59.874701
2274.239198	72243.218428	59.879706
2273.524964	72077.985128	59.884711
2272.758754	71897.849327	59.889716
2272.298493	71726.833004	59.894721
2271.980993	71550.563059	59.899725
2270.832372	71376.662634	59.904730
2270.230917	71196.684440	59.909735
2269.707914	71024.594583	59.914740
2268.928250	70850.526240	59.919745
2268.397551	70670.750648	59.924750
2267.603120	70509.704860	59.929754
2266.903547	70329.192711	59.934759
2266.462248	70165.078602	59.939764
2265.638214	69983.347854	59.944769
2265.255570	69808.414966	59.949774
2264.088632	69638.022886	59.954778
2263.612616	69461.594054	59.959783
2263.308513	69288.173507	59.964788
2262.442163	69105.038795	59.969793
2261.750345	68926.565155	59.974798
2260.809681	68760.521505	59.979802
2260.199150	68575.653716	59.984807
2259.796439	68419.921283	59.989812
2259.092108	68229.840029	59.994817
2258.358843	68066.125495	59.999822
2257.319882	67888.609443	60.004826
2256.790305	67732.199610	60.009831
2256.141397	67555.568412	60.014836
2255.395315	67388.827915	60.019841
2255.019582	67206.608550	60.024846
2254.087409	67034.029666	60.029850
2253.823069	66867.210903	60.034855
2252.852015	66696.123160	60.039860
2252.297017	66538.935341	60.044865
2251.885728	66348.176887	60.049870
2250.891357	66189.345363	60.054874
2250.349286	66005.095987	60.059879
2250.010758	65836.455016	60.064884
2249.120484	65664.135037	60.069889
2248.609506	65482.732308	60.074894
2247.616428	65315.741743	60.079898
2247.374414	65136.351400	60.084903
2246.819437	64959.824027	60.089908
2245.767480	64785.308521	60.094913
2245.394533	64605.795093	60.099918
2244.188418	64430.151609	60.104922
2243.501022	64261.389837	60.109927
2243.185921	64077.892324	60.114932
2242.312769	63917.170196	60.119937
2241.934717	63741.664475	60.124942
2241.133931	63572.439204	60.129946
2240.633265	63391.703688	60.134951
2239.957890	63222.866878	60.139956
2239.035769	63050.233568	60.144961
2238.733429	62873.644245	60.149966
2237.783238	62697.988796	60.154970
2236.769258	62534.726813	60.159975
2236.659116	62350.333325	60.164980
2236.059736	62184.368280	60.169985
2235.384426	62009.235961	60.174990
2234.778969	61839.380994	60.179994
2234.052673	61650.378257	60.184999
2233.295321	61469.736600	60.190004
2232.477325	61304.836480	60.195009
2231.704297	61124.244941	60.200014
2231.293896	60946.009800	60.205018
2230.824146	60790.913468	60.210023
2230.014144	60605.815489	60.215028
2229.366860	60429.474667	60.220033
2228.899921	60247.662253	60.225038
2228.528272	60068.780360	60.230042
2227.580343	59887.335799	60.235047
2226.784206	59707.483269	60.240052
2225.875764	59526.153068	60.245057
2225.541638	59347.234133	60.250062
2224.755676	59174.456481	60.255066
2224.370951	58997.935562	60.260071
2223.526729	58832.304855	60.265076
2222.739121	58640.199091	60.270081
2222.377187	58463.486542	60.275086
2221.476273	58288.282328	60.280090
2220.670050	58096.318073	60.285095
2220.251721	57933.913206	60.290100
2219.359209	57761.608694	60.295105
2218.785230	57564.799033	60.300110
2218.035575	57405.739824	60.305114
2217.616834	57213.394085	60.310119
2217.220729	57049.790755	60.315124
2216.170140	56872.382900	60.320129
2215.618362	56688.770407	60.325134
2214.906506	56504.928784	60.330138
2214.353588	56326.798434	60.335143
2213.773434	56154.367586	60.340148
2212.815824	55975.928224	60.345153
2212.480590	55800.635708	60.350158
2211.740106	55612.769349	60.355162
2210.986378	55437.489727	60.360167
2210.224679	55262.437734	60.365172
2209.444832	55084.311133	60.370177
2209.089233	54903.071475	60.375182
2208.190474	54736.002005	60.380186
2207.785413	54539.846638	60.385191
2207.145978	54364.929409	60.390196
2206.431532	54188.218856	60.395201
2205.810774	54011.226178	60.400206
2205.101804	53833.097377	60.405210
2204.470888	53653.410566	60.410215
2203.890656	53469.325405	60.415220
2202.837222	53295.170794	60.420225
2202.105092	53103.487489	60.425230
2201.296587	52939.543321	60.430234
2201.285117	52749.277756	60.435239
2200.083743	52592.135644	60.440244
2199.471352	52398.779611	60.445249
2199.006587	52217.634660	60.450254
2198.456478	52052.853852	60.455258
2197.752086	51871.608005	60.460263
2197.045109	51699.277423	60.465268
2196.284085	51510.251224	60.470273
2196.152949	51336.567163	60.475278
2194.618806	51158.291874	60.480282
2194.393517	50984.996323	60.485287
2193.768896	50803.359423	60.490292
2193.066664	50633.240352	60.495297
2192.608477	50457.152056	60.500302
2191.598682	50271.329510	60.505306
2191.278210	50090.635509	60.510311
2190.260680	49914.056006	60.515316
2189.820780	49730.246202	60.520321
2189.317295	49546.688815	60.525326
2188.266059	49380.648523	60.530330
2188.046032	49195.664116	60.535335
2187.182285	49018.240227	60.540340
2186.454183	48842.460594	60.545345
2185.844622	48663.035380	60.550350
2185.281519	48476.869627	60.555354
2185.013722	48301.882770	60.560359
2184.001979	48117.247139	60.565364
2183.066402	47944.508202	60.570369
2182.524311	47743.374677	60.575374
2181.669232	47579.091571	60.580378
2181.284975	47392.769648	60.585383
2180.792260	47217.917757	60.590388
2180.208347	47040.864670	60.595393
2179.426664	46860.238737	60.600398
2178.664370	46673.329614	60.605402
2178.190546	46482.353255	60.610407
2177.469365	46311.155693	60.615412
2176.194918	46126.607875	60.620417
2175.989945	45945.071126	60.625422
2174.946692	45774.613101	60.630426
2174.539638	45592.928604	60.635431
2174.146900	45405.151979	60.640436
2173.042799	45238.947102	60.645441
2172.496788	45053.197503	60.650446
2171.822120	44881.459355	60.655450
2171.300578	44692.958065	60.660455
2170.512208	44529.426663	60.665460
2169.740305	44345.320779	60.670465
2169.387295	44156.649898	60.675470
2168.723651	43995.690781	60.680474
2167.812630	43803.411974	60.685479
2167.374490	43635.184374	60.690484
2166.972958	43450.798323	60.695489
2166.121196	43265.454687	60.700494
2165.297664	43091.000118	60.705498
2164.500170	42899.560857	60.710503
2163.995178	42735.327780	60.715508
2163.346506	42542.376199	60.720513
2163.095705	42362.329245	60.725518
2162.066788	42191.546705	60.730522
2161.325289	42008.880678	60.735527
2160.815837	41822.732923	60.740532
2159.968174	41640.609413	60.745537
2159.269363	41464.402784	60.750542
2158.913376	41293.405377	60.755546
2158.255830	41100.224696	60.760551
2157.363121	40933.360371	60.765556
2156.814845	40748.678632	60.770561
2156.552892	40563.099707	60.775566
2155.436823	40380.361802	60.780570
2154.537759	40203.199128	60.785575
2153.904270	40022.891153	60.790580
2153.306278	39849.937142	60.795585
2152.805365	39669.629249	60.800590
2151.939824	39495.353782	60.805594
2151.411251	39320.160302	60.810599
2150.728585	39135.797124	60.815604
2149.915374	38964.596745	60.820609
2149.326999	38776.483768	60.825614
2148.859178	38608.442859	60.830618
2148.218898	38428.497448	60.835623
2147.805176	38249.605581	60.840628
2146.816255	38068.965263	60.845633
2146.157957	37888.269669	60.850638
2145.334230	37709.353714	60.855642
2145.200460	37521.729452	60.860647
2144.355490	37350.686345	60.865652
2143.434739	37168.475182	60.870657
2142.896899	36986.184680	60.875662
2142.098043	36807.671076	60.880666
2141.142520	36619.543898	60.885671
2140.867752	36452.209801	60.890676
2140.087945	36269.807380	60.895681
2139.646614	36094.753552	60.900686
2138.542450	35923.551101	60.905690
2138.120197	35738.937063	60.910695
2137.533278	35561.820814	60.915700
2136.842784	35387.585199	60.920705
2136.215980	35209.164010	60.925710
2135.416010	35044.889143	60.930714
2135.088621	34857.519705	60.935719
2134.281951	34672.224533	60.940724
2133.504628	34497.357659	60.945729
2133.019250	34316.116700	60.950734
2131.998609	34138.211957	60.955738
2131.465400	33964.590483	60.960743
2131.394047	33779.109536	60.965748
2130.338446	33600.563393	60.970753
2129.783245	33416.618769	60.975758
2128.715455	33241.594668	60.980762
2128.421282	33070.667490	60.985767
2127.619241	32890.285624	60.990772
2126.842456	32712.183624	60.995777
2126.503020	32518.793149	61.000782
2125.335514	32343.355051	61.005786
2124.853672	32173.655242	61.010791
2124.370828	31997.995231	61.015796
2123.190617	31823.756141	61.020801
2122.885738	31638.519498	61.025806
2122.049154	31469.377813	61.030810
2121.443858	31288.441802	61.035815
2120.852151	31118.724454	61.040820
2120.388200	30951.886492	61.045825
2119.474154	30765.438528	61.050830
2118.756562	30590.036193	61.055834
2118.388073	30408.283837	61.060839
2117.737179	30233.483048	61.065844
2117.023792	30072.305881	61.070849
2116.153230	29888.613376	61.075854
2115.940008	29711.712085	61.080858
2115.101428	29525.098779	61.085863
2114.444268	29351.092072	61.090868
2113.684184	29170.281412	61.095873
2113.038489	28982.659402	61.100878
2112.122245	28814.603661	61.105882
2111.478985	28642.014739	61.110887
2111.195888	28456.888009	61.115892
2110.347146	28288.223484	61.120897
2109.608197	28111.601494	61.125902
2108.890642	27944.351045	61.130906
2108.127587	27762.488546	61.135911
2107.582197	27583.821028	61.140916
2107.200443	27417.870269	61.145921
2106.536708	27234.572989	61.150926
2105.527600	27069.499428	61.155930
2104.914287	26887.140390	61.160935
2104.500508	26707.374031	61.165940
2103.418868	26542.483233	61.170945
2102.582341	26360.391458	61.175950
2102.164540	26197.334714	61.180954
2101.558582	26031.296345	61.185959
2100.890919	25849.640056	61.190964
2100.315378	25679.927899	61.195969
2099.972142	25496.813536	61.200974
2099.183788	25325.324756	61.205978
2098.439673	25149.166412	61.210983
2097.536950	24977.021882	61.215988
2096.769390	24800.240864	61.220993
2096.386779	24632.538036	61.225998
2095.249547	24459.719194	61.231002
2094.840320	24279.355369	61.236007
2094.244050	24114.290866	61.241012
2093.268943	23953.983803	61.246017
2092.680992	23780.069579	61.251022
2092.136987	23606.289264	61.256026
2091.204065	23447.559192	61.261031
2090.843324	23274.809216	61.266036
2089.930687	23104.687478	61.271041
2089.188830	22927.699640	61.276046
2088.552945	22774.078518	61.281050
2088.134062	22602.152885	61.286055
2087.364533	22439.057601	61.291060
2086.449042	22275.797646	61.296065
2086.169035	22102.324304	61.301070
2085.290189	21931.563080	61.306074
2085.000957	21771.449495	61.311079
2084.576749	21592.654279	61.316084
2083.684421	21429.872338	61.321089
2083.064304	21250.538844	61.326094
2082.155127	21093.354822	61.331098
2082.058149	20914.400073	61.336103
2081.218754	20748.752240	61.341108
2080.215481	20580.798270	61.346113
2079.848669	20396.117123	61.351118
2078.844020	20229.644336	61.356122
2077.886407	20070.466899	61.361127
2077.433282	19901.245052	61.366132
2076.803797	19734.916531	61.371137
2076.102038	19564.017457	61.376142
2075.555341	19398.814254	61.381146
2075.003245	19228.080620	61.386151
2074.102842	19065.807591	61.391156
2073.340756	18904.053888	61.396161
2072.719359	18734.857523	61.401166
2071.851217	18577.965325	61.406170
2071.358216	18418.710811	61.411175
2070.990188	18249.638957	61.416180
2069.912291	18088.920337	61.421185
2069.222718	17920.819986	61.426190
2068.480924	17775.748644	61.431194
2067.792181	17610.769641	61.436199
2067.144157	17455.787424	61.441204
2066.197861	17299.562669	61.446209
2065.743772	17138.116662	61.451214
2065.078099	16983.089468	61.456218
2064.315183	16821.442579	61.461223
2063.591012	16675.899772	61.466228
2062.953795	16513.308470	61.471233
2062.262980	16363.988495	61.476238
2061.213635	16213.117043	61.481242
2060.690489	16059.721612	61.486247
2060.015284	15917.315098	61.491252
2059.064789	15781.879883	61.496257
2058.411139	15627.398124	61.501262
2058.150167	15475.083441	61.506266
2057.293025	15345.951015	61.511271
2056.413894	15194.048585	61.516276
2055.600734	15059.379201	61.521281
2054.941486	14922.136976	61.526286
2053.792508	14792.681502	61.531290
2052.941492	14661.170813	61.536295
2052.099055	14541.603093	61.541300
2050.442058	14442.711907	61.546305
2049.476726	14339.222767	61.551310
2047.752102	14252.473943	61.556314
2046.695202	14179.307834	61.561319
2045.810742	14088.573737	61.566324
2044.919053	14021.889489	61.571329
2044.124093	13952.624967	61.576334
2043.167375	13898.480910	61.581338
2042.573395	13825.117911	61.586343
2041.906189	13771.714397	61.591348
2040.775711	13715.996302	61.596353
2040.226856	13655.921018	61.601358
2039.852322	13622.770640	61.606362
2039.090247	13561.687840	61.611367
2038.258199	13509.408867	61.616372
2037.940884	13451.271187	61.621377
2037.401733	13398.947856	61.626382
2036.745472	13350.191247	61.631386
2036.105490	13280.514141	61.636391
2035.551550	13234.406395	61.641396
2034.860741	13180.052818	61.646401
2034.352427	13124.649589	61.651406
2034.016297	13075.092457	61.656410
2033.361162	13005.337927	61.661415
2032.628311	12960.483587	61.666420
2031.950198	12893.772248	61.671425
2031.911842	12826.167947	61.676430
2031.214637	12775.924734	61.681434
2030.235461	12718.561626	61.686439
2029.845520	12650.223386	61.691444
2028.763114	12588.504934	61.696449
2028.390746	12519.720603	61.701454
2027.213665	12468.112635	61.706458
2026.947731	12406.947925	61.711463
2026.470062	12354.392859	61.716468
2025.688883	12297.449320	61.721473
2025.479931	12224.109854	61.726478
2024.738082	12173.640957	61.731482
2024.222701	12117.168041	61.736487
2023.515336	12042.501379	61.741492
2022.860617	11985.908437	61.746497
2022.207778	11915.256400	61.751502
2021.433543	11851.570575	61.756506
2020.691081	11785.863841	61.761511
2019.864914	11726.101479	61.766516
2019.174040	11680.074632	61.771521
2018.899599	11603.163731	61.776526
2018.188482	11552.923029	61.781530
2017.259734	11490.961742	61.786535
2016.767344	11424.001705	61.791540
2016.117080	11368.188588	61.796545
2015.673119	11300.763352	61.801550
2014.980230	11241.001478	61.806554
2014.434248	11168.020651	61.811559
2013.651108	11114.783356	61.816564
2012.790533	11051.768336	61.821569
2012.250697	10981.951937	61.826574
2011.094661	10923.601881	61.831578
2010.568678	10873.307223	61.836583
2010.277192	10808.547075	61.841588
2009.548884	10752.648016	61.846593
2008.827825	10691.378621	61.851598
2007.850662	10634.337525	61.856602
2007.591593	10573.432007	61.861607
2006.927847	10518.179056	61.866612
2006.364537	10465.276058	61.871617
2005.462387	10395.544340	61.876622
2004.676395	10338.610915	61.881626
2004.408135	10278.557423	61.886631
2003.919661	10214.465457	61.891636
2002.976374	10162.851537	61.896641
2002.782724	10096.300488	61.901646
2001.536781	10040.967922	61.906650
2000.687417	9985.387591	61.911655
2000.474307	9929.636645	61.916660
1999.531665	9875.213994	61.921665
1999.165494	9809.638782	61.926670
1998.576072	9748.379153	61.931674
1997.847283	9683.340177	61.936679
1997.221345	9629.444498	61.941684
1996.475661	9573.816883	61.946689
1995.939357	9512.464969	61.951694
1995.322964	9446.612706	61.956698
1994.832163	9381.116345	61.961703
1993.866207	9313.486199	61.966708
1993.021218	9259.452652	61.971713
1992.449853	9193.306383	61.976718
1991.841257	9136.225093	61.981722
1991.379361	9078.040263	61.986727
1991.022422	9007.859998	61.991732
1990.064115	8949.242834	61.996737
1989.203343	8890.503121	62.001742
1988.795261	8834.901579	62.006746
1987.771603	8765.056287	62.011751
1986.976685	8699.385541	62.016756
1986.260926	8660.806185	62.021761
1986.398210	8596.870299	62.026766
1985.521096	8531.157325	62.031770
1984.327712	8475.557519	62.036775
1984.385198	8414.162385	62.041780
1983.540006	8354.925285	62.046785
1983.557185	8289.813779	62.051790
1982.103455	8221.290903	62.056794
1981.567670	8159.245867	62.061799
1981.304056	8096.593819	62.066804
1980.242166	8042.406608	62.071809
1979.776375	7967.764402	62.076814
1979.013049	7913.482142	62.081818
1978.179727	7843.788443	62.086823
1977.550197	7783.646077	62.091828
1976.802635	7727.923855	62.096833
1976.306126	7662.467471	62.101838
1975.406898	7604.202781	62.106842
1974.969879	7531.466475	62.111847
1974.276831	7457.955478	62.116852
1973.347521	7416.636429	62.121857
1973.049193	7344.942405	62.126862
1972.444235	7280.622728	62.131866
1971.481063	7224.602141	62.136871
1970.807284	7159.297984	62.141876
1970.099003	7108.278131	62.146881
1969.566738	7037.240391	62.151886
1968.905206	6992.637075	62.156890
1968.113543	6933.426314	62.161895
1967.897666	6870.747380	62.166900
1966.935215	6807.456766	62.171905
1966.330652	6745.074347	62.176910
1965.422947	6687.925264	62.181914
1964.549919	6629.942632	62.186919
1963.910933	6566.790225	62.191924
1963.428359	6515.180460	62.196929
1962.740849	6449.568047	62.201934
1962.014922	6399.813952	62.206938
1961.104189	6339.823818	62.211943
1960.923672	6278.400704	62.216948
1960.071703	6234.026312	62.221953
1959.908504	6179.378244	62.226958
1959.184858	6114.980698	62.231962
1958.585750	6051.242811	62.236967
1957.765987	6002.315037	62.241972
1956.884374	5933.127799	62.246977
1956.393933	5862.959855	62.251982
1955.203934	5826.302580	62.256986
1954.614285	5766.945302	62.261991
1954.500975	5706.476192	62.266996
1953.627544	5643.611033	62.272001
1953.007255	5588.337278	62.277006
1952.632860	5534.193643	62.282010
1951.864975	5473.361662	62.287015
1951.000757	5410.888833	62.292020
1950.280395	5368.374969	62.297025
1949.653488	5293.881398	62.302030
1949.079107	5245.684630	62.307034
1948.197645	5190.061819	62.312039
1947.687856	5124.347400	62.317044
1947.135539	5078.233901	62.322049
1946.306093	5001.737429	62.327054
1945.390147	4961.648025	62.332058
1944.990956	4896.530698	62.337063
1944.286173	4842.917650	62.342068
1943.675865	4790.028045	62.347073
1943.132344	4718.780783	62.352078
1942.537524	4662.361228	62.357082
1941.613355	4612.973517	62.362087
1941.393212	4547.494889	62.367092
1940.556837	4491.518946	62.372097
1939.991612	4435.116068	62.377102
1939.115976	4385.705642	62.382106
1938.559996	4330.252087	62.387111
1937.809581	4264.873883	62.392116
1937.018143	4224.295871	62.397121
1936.621438	4147.980414	62.402126
1935.797203	4095.454574	62.407130
1935.267173	4036.821958	62.412135
1934.668005	3984.557328	62.417140
1933.997357	3916.674985	62.422145
1933.387653	3851.113025	62.427150
1932.631853	3807.018541	62.432154
1931.926733	3742.811378	62.437159
1931.047128	3689.534715	62.442164
1930.080034	3631.205763	62.447169
1929.784222	3567.699387	62.452174
1929.152191	3522.920479	62.457178
1928.672566	3467.667050	62.462183
1928.074864	3404.509785	62.467188
1927.425806	3355.030579	62.472193
1926.893042	3291.254656	62.477198
1925.768142	3231.713387	62.482202
1925.187743	3171.626138	62.487207
1924.554795	3122.667238	62.492212
1923.989949	3070.158304	62.497217
1923.277159	3005.812843	62.502222
1922.664174	2951.528887	62.507226
1921.687677	2896.957427	62.512231
1921.292233	2828.772236	62.517236
1920.367731	2785.721777	62.522241
1920.214893	2724.182091	62.527246
1919.334032	2669.192528	62.532250
1918.634761	2626.123341	62.537255
1918.349211	2563.301042	62.542260
1917.241665	2513.690859	62.547265
1916.681371	2456.824795	62.552270
1915.920308	2392.834313	62.557274
1915.371256	2331.397036	62.562279
1914.894186	2277.956722	62.567284
1914.058990	2229.171717	62.572289
1913.534309	2163.820669	62.577294
1912.549267	2114.827993	62.582298
1911.790219	2057.160722	62.587303
1911.459407	1998.811389	62.592308
1910.546849	1957.695066	62.597313
1909.899975	1889.476105	62.602318
1908.952657	1836.912464	62.607322
1908.282440	1792.866458	62.612327
1907.915319	1743.471751	62.617332
1907.433724	1693.195640	62.622337
1906.692298	1631.910136	62.627342
1905.757707	1585.003272	62.632346
1904.799975	1523.982034	62.637351
1904.403079	1472.400805	62.642356
1903.511259	1425.462432	62.647361
1902.839929	1381.278276	62.652366
1902.682247	1329.606740	62.657370
1901.952809	1279.461303	62.662375
1901.363501	1232.416383	62.667380
1900.386409	1172.140129	62.672385
1900.264170	1124.671292	62.677390
1899.254075	1082.661395	62.682394
1898.546886	1023.114085	62.687399
1897.896696	970.596295	62.692404
1897.123052	930.194149	62.697409
1896.655077	868.059428	62.702414
1896.057353	831.313566	62.707418
1895.200653	773.582518	62.712423
1894.827116	721.518463	62.717428
1893.775038	677.191892	62.722433
1893.033141	628.569340	62.727438
1892.536047	578.204137	62.732442
1891.666586	535.487505	62.737447
1891.440103	484.120062	62.742452
1890.338125	440.114384	62.747457
1889.465012	383.653812	62.752462
1888.714369	340.226599	62.757466
1888.108460	299.750695	62.762471
1887.351584	255.820096	62.767476
1886.725030	217.998572	62.772481
1886.243428	170.966802	62.777486
1885.439988	138.464249	62.782490
1884.546828	106.825990	62.787495
1884.140957	50.265723	62.792500
1883.139494	20.885680	62.797505
1882.674722	-6.184157	62.802510
1881.659911	-50.804566	62.807514
1880.866216	-74.999345	62.812519
1880.013350	-102.904649	62.817524
1876.847317	-50.240243	62.822529
1873.891304	3.015472	62.827534
1874.132242	-3.341411	62.832538
1874.617201	2.142002	62.837543
1875.002392	-2.427466	62.842548
1874.752417	1.143128	62.847553
1874.401274	-7.575027	62.852558
1874.215794	-0.261572	62.857562
1872.557525	2.070819	62.862567
1871.656153	-2.682290	62.867572
1870.906270	6.419144	62.872577
1870.111314	0.412821	62.877582
1869.939364	11.508776	62.882586
1869.168607	8.680863	62.887591
1868.985692	11.496499	62.892596
1867.983630	13.688429	62.897601
1867.095606	8.050115	62.902606
1867.086847	12.772997	62.907610
1866.384012	24.071528	62.912615
1866.048344	11.233525	62.917620
1864.258756	24.710481	62.922625
1864.061346	13.395921	62.927630
1863.665191	15.034331	62.932634
1862.792782	17.521063	62.937639
1862.271520	16.397625	62.942644
1861.398890	19.231319	62.947649
1860.682561	10.563258	62.952654
1860.147119	11.641897	62.957658
1860.080254	19.135221	62.962663
1859.775131	15.433866	62.967668
1858.097643	25.980426	62.972673
1857.350184	18.447968	62.977678
1857.155685	20.164744	62.982682
1856.776735	21.281613	62.987687
1856.014958	16.159412	62.992692
1854.670709	22.253406	62.997697
1854.660333	22.580051	63.002702
1853.636211	25.988154	63.007706
1853.135345	18.284079	63.012711
1852.575477	20.940380	63.017716
1851.507945	20.438268	63.022721
1851.109491	17.522856	63.027726
1850.474853	18.342862	63.032730
1849.354112	20.069525	63.037735
1849.254001	11.973815	63.042740
1848.338767	28.450042	63.047745
1847.929718	13.595754	63.052750
1847.081795	9.622631	63.057754
1846.409503	15.868542	63.062759
1845.938655	13.754672	63.067764
1845.278624	18.234047	63.072769
1845.036379	14.527440	63.077774
1844.162127	17.490705	63.082778
1843.310710	28.182063	63.087783
1842.886332	11.061002	63.092788
1841.957559	30.686944	63.097793
1841.545261	16.427676	63.102798
1840.770705	18.968262	63.107802
1839.925179	21.386079	63.112807
1839.389179	27.785393	63.117812
1838.785498	29.076721	63.122817
1838.379098	18.340970	63.127822
1837.437785	17.183316	63.132826
1836.797177	24.031321	63.137831
1836.404886	17.442249	63.142836
1835.626181	20.710462	63.147841
1834.975116	20.389802	63.152846
1833.720959	27.185431	63.157850
1833.361440	14.513646	63.162855
1833.178646	15.347058	63.167860
1831.744190	22.791052	63.172865
1831.765682	10.304769	63.177870
1830.737865	21.427832	63.182874
1829.783972	28.208896	63.187879
1829.971006	13.184264	63.192884
1828.681669	23.568275	63.197889
1828.052518	23.072251	63.202894
1827.469649	17.793917	63.207898
1826.792618	25.759447	63.212903
1825.980603	24.820959	63.217908
1825.311203	27.458390	63.222913
1825.475918	27.575882	63.227918
1824.691201	14.533234	63.232922
1823.646858	24.638648	63.237927
1823.343812	19.777920	63.242932
1822.557577	22.742985	63.247937
1822.265897	23.063839	63.252942
1821.105197	24.694360	63.257946
1819.690718	20.098440	63.262951
1819.459190	17.022486	63.267956
1819.203129	11.917759	63.272961
1818.611023	18.199827	63.277966
1817.717730	22.883408	63.282970
1817.166259	19.874031	63.287975
1816.799145	17.530806	63.292980
1815.699694	21.002924	63.297985
1815.249298	17.299414	63.302990
1814.697294	8.266235	63.307994
1813.902247	12.834864	63.312999
1812.926685	28.973752	63.318004
1811.842633	21.603572	63.323009
1811.946228	15.375721	63.328014
1811.511756	11.828956	63.333018
1810.126489	20.359540	63.338023
1809.486614	15.083957	63.343028
1808.729153	26.208248	63.348033
1808.532845	9.613948	63.353038
1808.214671	12.791685	63.358042
1807.508698	21.195469	63.363047
1807.242772	17.383819	63.368052
1806.311742	22.114396	63.373057
1805.267019	13.091657	63.378062
1804.295511	14.469790	63.383066
1803.610319	19.413635	63.388071
1803.281062	17.002900	63.393076
1802.467419	15.626290	63.398081
1802.261263	12.722926	63.403086
1801.632214	19.094442	63.408090
1800.735930	18.517847	63.413095
1800.417807	16.666733	63.418100
1799.369963	21.149361	63.423105
1798.508250	16.740056	63.428110
1797.985880	25.120994	63.433114
1797.106128	18.817501	63.438119
1796.981901	6.882641	63.443124
1796.114893	8.652606	63.448129
1795.564636	15.129878	63.453134
1794.904929	15.118103	63.458138
1793.674435	26.412137	63.463143
1793.117642	16.055095	63.468148
1792.391560	18.960152	63.473153
1792.243622	26.784892	63.478158
1791.588688	17.698676	63.483162
1790.809098	23.926949	63.488167
1790.631919	19.446778	63.493172
1789.905256	31.338884	63.498177
1788.883940	15.030146	63.503182
1787.670316	24.481220	63.508186
1786.859042	17.162348	63.513191
1786.851109	20.639320	63.518196
1785.913913	32.427669	63.523201
1785.552010	13.603074	63.528206
1785.144506	23.440204	63.533210
1784.503196	26.730765	63.538215
1784.002710	18.205065	63.543220
1782.687313	24.542090	63.548225
1781.727077	24.626932	63.553230
1781.366726	19.641273	63.558234
1780.725780	26.139263	63.563239
1780.556599	23.247373	63.568244
1779.870069	16.708199	63.573249
1779.432631	10.340776	63.578254
1778.195423	12.727778	63.583258
1777.219505	27.911106	63.588263
1776.783708	7.872979	63.593268
1776.101958	18.379704	63.598273
1775.866056	15.197218	63.603278
1775.378584	16.235139	63.608282
1774.545450	22.241687	63.613287
1773.621220	22.593623	63.618292
1772.426330	26.249648	63.623297
1772.297571	24.327462	63.628302
1771.542142	17.745617	63.633306
1771.061414	23.516425	63.638311
1771.141540	14.239359	63.643316
1769.796856	18.480562	63.648321
1768.450314	12.494068	63.653326
1767.883337	13.368001	63.658330
1767.125082	19.189194	63.663335
1767.469360	13.971781	63.668340
1766.602419	23.378838	63.673345
1766.086821	17.321870	63.678350
1765.850825	17.417847	63.683354
1764.230125	24.460950	63.688359
1763.927543	12.872959	63.693364
1762.868298	11.404485	63.698369
1762.323999	13.403901	63.703374
1762.085677	7.082130	63.708378
1761.213561	31.220152	63.713383
1760.790073	12.512580	63.718388
1759.256803	27.114237	63.723393
1758.454412	24.001226	63.728398
1758.258649	17.888730	63.733402
1757.524276	12.481518	63.738407
1757.422399	24.580315	63.743412
1756.763585	24.109520	63.748417
1756.221625	21.355687	63.753422
1755.849542	22.428901	63.758426
1754.573219	17.847347	63.763431
1754.140288	14.722966	63.768436
1753.435893	16.790390	63.773441
1752.380906	23.294221	63.778446
1751.469747	22.098694	63.783450
1750.568582	18.206600	63.788455
1750.658351	20.423851	63.793460
1749.958154	22.375494	63.798465
1749.270785	10.493814	63.803470
1748.844514	12.851373	63.808474
1748.356110	12.955903	63.813479
1747.644028	5.569259	63.818484
1746.574635	14.688354	63.823489
1745.947139	19.703471	63.828494
1745.317145	11.715590	63.833498
1744.847133	16.309882	63.838503
1744.477587	4.257881	63.843508
1742.940910	16.204522	63.848513
1742.732439	9.480624	63.853518
1742.040821	17.150441	63.858522
1741.324719	11.551101	63.863527
1741.027032	11.899726	63.868532
1739.812090	15.262483	63.873537
1739.099688	11.537530	63.878542
1738.591696	4.681439	63.883546
1737.869193	21.866645	63.888551
1737.533746	6.059281	63.893556
1737.066310	21.715350	63.898561
1736.078550	14.848727	63.903566
1735.186843	19.784388	63.908570
1734.182090	16.298256	63.913575
1733.876097	12.464598	63.918580
1732.928193	14.890822	63.923585
1732.936321	12.068546	63.928590
1732.636267	13.543477	63.933594
1731.887593	10.109713	63.938599
1731.289482	13.606307	63.943604
1730.121208	16.032843	63.948609
1729.643866	10.045504	63.953614
1728.906349	19.578665	63.958618
1727.966495	19.184056	63.963623
1727.161431	10.441831	63.968628
1726.365846	18.435668	63.973633
1726.033773	8.752579	63.978638
1725.865640	14.322351	63.983642
1725.243049	7.691043	63.988647
1724.574750	0.679073	63.993652
1723.620856	17.248180	63.998657
1723.218400	9.755592	64.003662
1722.906674	14.023550	64.008666
1721.675771	20.044407	64.013671
1720.491266	4.280453	64.018676
1720.185656	21.675404	64.023681
1719.468518	11.596168	64.028686
1719.204795	5.322592	64.033690
1718.419635	16.864448	64.038695
1717.467717	6.876125	64.043700
1716.353156	23.842917	64.048705
1716.255352	7.430114	64.053710
1715.629008	3.442345	64.058714
1714.831445	16.395948	64.063719
1714.557941	12.520862	64.068724
1714.081016	12.822268	64.073729
1712.913751	13.313754	64.078734
1712.457414	4.812609	64.083738
1711.410498	21.312922	64.088743
1711.179629	4.454487	64.093748
1710.378018	9.279647	64.098753
1709.984263	11.043851	64.103758
1709.029171	9.681856	64.108762
1708.346588	9.506582	64.113767
1708.144817	18.200871	64.118772
1707.027221	8.792373	64.123777
1706.055367	8.611010	64.128782
1705.375069	9.348417	64.133786
1704.655387	15.053110	64.138791
1704.639420	7.704136	64.143796
1703.867259	15.214868	64.148801
1703.703883	1.802354	64.153806
1702.329808	16.735124	64.158810
1701.363727	14.693642	64.163815
1701.305623	8.398445	64.168820
1700.848630	10.896507	64.173825
1699.948280	6.263148	64.178830
1698.807454	4.796623	64.183834
1698.233136	11.000188	64.188839
1697.644277	11.264185	64.193844
1697.269501	22.870168	64.198849
1696.769135	11.529653	64.203854
1696.534560	10.892136	64.208858
1695.038549	19.206975	64.213863
1694.916509	14.673905	64.218868
1693.808588	13.145384	64.223873
1693.100587	19.269266	64.228878
1692.117451	13.947323	64.233882
1691.216843	16.006508	64.238887
1690.848993	3.466982	64.243892
1690.408531	11.431218	64.248897
1690.028251	14.620408	64.253902
1690.125536	5.391089	64.258906
1688.777105	18.966785	64.263911
1687.976601	2.414888	64.268916
1687.268281	19.634113	64.273921
1686.720413	16.914352	64.278926
1686.059645	5.608786	64.283930
1684.889297	8.015170	64.288935
1684.513856	18.192554	64.293940
1683.460171	8.586261	64.298945
1682.991593	11.319552	64.303950
1682.931026	18.092784	64.308954
1682.385622	18.504421	64.313959
1681.517810	14.479324	64.318964
1680.359495	10.522455	64.323969
1680.064475	11.376858	64.328974
1679.574825	12.489258	64.333978
1678.840677	4.257755	64.338983
1677.695570	15.131409	64.343988
1677.029551	11.846956	64.348993
1676.417724	20.317808	64.353998
1676.113090	10.888987	64.359002
1675.511710	8.508887	64.364007
1675.237183	8.787608	64.369012
1674.020376	8.998403	64.374017
1673.159354	7.195707	64.379022
1672.761940	0.987534	64.384026
1672.019039	4.830410	64.389031
1671.962222	7.171865	64.394036
1670.789238	11.264413	64.399041
1669.829283	8.972816	64.404046
1669.644971	13.050227	64.409050
1669.024035	9.265035	64.414055
1667.668090	-0.897191	64.419060
1666.769824	11.523642	64.424065
1666.316951	-0.751635	64.429070
1666.017885	7.521294	64.434074
1665.463824	11.826176	64.439079
1665.132454	11.245040	64.444084
1664.447279	7.862710	64.449089
1663.960933	21.454427	64.454094
1662.829244	13.423273	64.459098
1661.945459	18.867045	64.464103
1661.685840	13.999448	64.469108
1661.050837	16.666143	64.474113
1659.872829	22.915163	64.479118
1659.141215	14.730567	64.484122
1658.410221	21.772731	64.489127
1658.222116	19.189785	64.494132
1657.969691	15.241974	64.499137
1657.380694	19.079330	64.504142
1656.251553	9.133381	64.509146
1655.232284	21.040445	64.514151
1655.195306	16.949597	64.519156
1654.550072	11.544029	64.524161
1653.673869	16.765828	64.529166
1652.953969	10.771311	64.534170
1651.811492	20.463438	64.539175
1651.776705	9.947824	64.544180
1651.311006	19.043582	64.549185
1650.412961	12.022400	64.554190
1649.780481	15.292661	64.559194
1648.920946	16.433868	64.564199
1648.399337	15.794649	64.569204
1647.749641	24.033407	64.574209
1646.408651	20.111881	64.579214
1645.978097	15.135826	64.584218
1645.232082	18.939783	64.589223
1645.057278	16.118186	64.594228
1644.703805	11.191387	64.599233
1643.967542	14.522292	64.604238
1643.484365	15.338784	64.609242
1642.264980	9.308509	64.614247
1642.190859	13.029375	64.619252
1641.004725	11.943806	64.624257
1640.175254	16.087447	64.629262
1639.769780	9.804865	64.634266
1639.018016	9.318907	64.639271
1639.005031	8.654076	64.644276
1637.852320	14.139001	64.649281
1636.843279	9.507165	64.654286
1636.632188	4.510441	64.659290
1635.924657	19.677959	64.664295
1635.434118	6.834666	64.669300
1634.197424	13.466748	64.674305
1633.593668	12.474735	64.679310
1633.278484	15.447012	64.684314
1632.610732	18.836420	64.689319
1631.918390	14.748773	64.694324
1630.765130	16.803963	64.699329
1630.219167	12.156904	64.704334
1629.833852	20.113965	64.709338
1629.313895	21.428306	64.714343
1628.840203	19.135161	64.719348
1627.802295	16.707733	64.724353
1626.793382	23.798790	64.729358
1626.544688	4.964160	64.734362
1625.992980	13.395502	64.739367
1625.738513	10.767912	64.744372
1624.426752	9.479963	64.749377
1623.659534	23.214077	64.754382
1623.240613	13.147420	64.759386
1622.740570	8.559300	64.764391
1622.443370	12.279338	64.769396
1621.163861	19.959005	64.774401
1620.622749	12.367046	64.779406
1620.476852	17.364015	64.784410
1619.074187	11.599412	64.789415
1618.417899	5.178493	64.794420
1617.694617	18.874085	64.799425
1617.441164	15.353790	64.804430
1616.870069	16.554834	64.809434
1615.744019	12.364215	64.814439
1615.132862	13.387123	64.819444
1614.736734	17.908193	64.824449
1614.134963	18.383992	64.829454
1613.968270	10.787740	64.834458
1612.893143	13.973799	64.839463
1612.323092	3.059122	64.844468
1611.532959	18.682882	64.849473
1610.314327	17.526797	64.854478
1609.976227	9.945165	64.859482
1609.017248	15.504975	64.864487
1608.854583	18.590214	64.869492
1608.205600	7.386882	64.874497
1607.157794	20.189457	64.879502
1606.657443	8.699162	64.884506
1605.659433	14.410252	64.889511
1605.386991	11.116901	64.894516
1604.732444	13.960176	64.899521
1604.355203	17.864820	64.904526
1603.762516	17.692636	64.909530
1602.804651	17.901746	64.914535
1602.415564	9.943445	64.919540
1601.595394	18.354371	64.924545
1600.277105	19.847600	64.929550
1599.923676	3.844444	64.934554
1599.041110	18.601389	64.939559
1599.054477	14.668124	64.944564
1598.618400	22.631677	64.949569
1597.781658	16.427087	64.954574
1596.983841	13.997794	64.959578
1596.150354	21.511988	64.964583
1595.619858	9.786792	64.969588
1594.355535	19.674913	64.974593
1593.507179	18.682351	64.979598
1592.980681	8.990762	64.984602
1592.880272	17.170633	64.989607
1592.636243	6.273543	64.994612
1592.388042	15.986018	64.999617
1591.419845	10.846248	65.004622
1591.017760	8.343041	65.009626
1589.297308	11.168028	65.014631
1588.854390	7.800844	65.019636
1588.297761	0.927293	65.024641
1587.079815	15.811642	65.029646
1586.996308	2.115230	65.034650
1586.281565	13.675879	65.039655
1585.647486	16.080673	65.044660
1585.114586	13.648714	65.049665
1584.456209	12.499815	65.054670
1584.068489	11.866143	65.059674
1582.592491	12.789937	65.064679
1582.094660	8.799131	65.069684
1581.343910	14.079862	65.074689
1580.673865	17.591070	65.079694
1580.644310	2.285501	65.084698
1580.077076	7.182261	65.089703
1578.938652	9.766540	65.094708
1577.971582	11.136165	65.099713
1577.591474	10.797748	65.104718
1577.462580	-0.582823	65.109722
1576.200260	4.654615	65.114727
1575.649505	12.560694	65.119732
1575.139180	14.493247	65.124737
1574.538215	15.870931	65.129742
1574.152806	4.945850	65.134746
1572.853327	8.765228	65.139751
1572.071174	3.315213	65.144756
1572.012227	-0.373170	65.149761
1571.364431	10.490877	65.154766
1570.538440	0.667119	65.159770
1569.489631	7.960065	65.164775
1569.191865	5.255786	65.169780
1568.791059	15.818820	65.174785
1567.732319	12.711918	65.179790
1567.351032	9.234022	65.184794
1566.403752	6.826914	65.189799
1566.175497	11.852737	65.194804
1565.098263	8.849700	65.199809
1563.890951	19.725393	65.204814
1563.956416	7.035044	65.209818
1562.993447	17.875063	65.214823
1562.651411	13.326502	65.219828
1561.699534	11.099896	65.224833
1560.699581	10.303320	65.229838
1560.417223	15.955898	65.234842
1559.876397	15.122634	65.239847
1559.367649	6.680320	65.244852
1558.847383	11.344120	65.249857
1557.722767	5.689912	65.254862
1557.538718	4.000453	65.259866
1556.769344	7.267255	65.264871
1556.045192	13.442614	65.269876
1555.234189	8.995385	65.274881
1554.237522	8.879523	65.279886
1554.188169	10.540135	65.284890
1553.517816	19.062881	65.289895
1552.714436	3.709973	65.294900
1552.012882	5.486839	65.299905
1551.241293	14.017785	65.304910
1550.639947	9.297548	65.309914
1549.668378	8.464928	65.314919
1549.198480	10.769524	65.319924
1548.603488	9.476523	65.324929
1548.311863	11.819021	65.329934
1547.604201	12.327432	65.334938
1546.203690	14.346256	65.339943
1545.679906	8.268574	65.344948
1545.374863	7.352115	65.349953
1544.937941	9.394432	65.354958
1544.426433	5.837888	65.359962
1543.102348	15.065328	65.364967
1542.714312	6.390950	65.369972
1542.372662	5.060846	65.374977
1541.183064	12.369868	65.379982
1540.620116	5.424794	65.384986
1539.805536	12.743608	65.389991
1539.402087	1.977521	65.394996
1539.027059	12.110686	65.400001
1538.103045	7.654614	65.405006
1537.432820	3.678601	65.410010
1536.626728	1.890878	65.415015
1536.020093	5.280055	65.420020
1535.763351	-0.482094	65.425025
1534.476493	-5.930733	65.430030
1534.275126	8.732154	65.435034
1533.385344	2.753640	65.440039
1533.159941	1.676297	65.445044
1531.996630	9.015836	65.450049
1531.084221	2.570994	65.455054
1530.939986	3.325757	65.460058
1530.227146	9.950325	65.465063
1529.623014	6.484196	65.470068
1528.898076	8.474516	65.475073
1528.215946	2.735814	65.480078
1527.843982	4.545463	65.485082
1526.575636	8.413530	65.490087
1525.970631	8.156591	65.495092
1525.265301	6.545245	65.500097
1524.890342	6.075132	65.505102
1524.783851	-3.158056	65.510106
1523.618045	9.308475	65.515111
1522.776476	3.651881	65.520116
1522.291731	3.131408	65.525121
1521.959252	14.058893	65.530126
1521.162748	5.331165	65.535130
1520.195206	3.674759	65.540135
1519.733662	4.027372	65.545140
1519.271587	6.428498	65.550145
1517.852049	-2.028327	65.555150
1517.805680	3.823284	65.560154
1516.633721	15.145950	65.565159
1516.279753	-0.950127	65.570164
1515.858859	4.885311	65.575169
1514.843127	5.521536	65.580174
1514.415530	4.135710	65.585178
1513.722552	16.803070	65.590183
1513.083347	8.225384	65.595188
1512.174724	6.165386	65.600193
1511.385004	3.386336	65.605198
1511.003189	0.943002	65.610202
1510.277316	3.876477	65.615207
1509.698866	3.225821	65.620212
1508.533117	10.829104	65.625217
1507.987163	1.307793	65.630222
1507.738182	-1.232343	65.635226
1507.267933	5.542904	65.640231
1506.854683	-1.403870	65.645236
1506.032740	3.088686	65.650241
1505.152849	9.094843	65.655246
1504.802991	4.820347	65.660250
1503.544638	14.352741	65.665255
1502.916000	-0.231560	65.670260
1502.137648	0.330674	65.675265
1501.527584	6.658218	65.680270
1501.572599	0.081731	65.685274
1500.288275	16.727046	65.690279
1499.954359	3.215524	65.695284
1499.080611	3.696727	65.700289
1498.425725	9.047393	65.705294
1498.000421	-1.322551	65.710298
1496.642121	-0.426876	65.715303
1496.722763	-3.252783	65.720308
1496.216904	2.283929	65.725313
1495.382800	7.915387	65.730318
1494.419344	7.168229	65.735322
1493.528188	14.213800	65.740327
1493.281353	9.702162	65.745332
1492.792901	1.918953	65.750337
1491.470696	6.554098	65.755342
1491.150195	-0.557222	65.760346
1490.538972	0.770071	65.765351
1490.363944	11.000759	65.770356
1489.085430	-0.247548	65.775361
1488.206708	6.632045	65.780366
1487.884639	1.287133	65.785370
1487.337697	5.802220	65.790375
1486.758462	3.382381	65.795380
1485.910352	4.250592	65.800385
1485.093020	13.116821	65.805390
1485.006369	6.770989	65.810394
1483.909640	16.876938	65.815399
1483.081441	3.120708	65.820404
1482.527532	8.909484	65.825409
1481.964731	11.413357	65.830414
1482.022624	-0.406885	65.835418
1480.652418	7.593172	65.840423
1479.728591	2.820134	65.845428
1479.227868	7.495031	65.850433
1478.601084	3.926863	65.855438
1478.195577	5.861696	65.860442
1476.858310	10.562319	65.865447
1476.598687	-1.838227	65.870452
1476.265826	3.002375	65.875457
1475.572419	6.673432	65.880462
1474.847787	3.660126	65.885466
1474.080030	4.545531	65.890471
1473.503994	3.569653	65.895476
1472.368677	5.864904	65.900481
1471.465102	7.733823	65.905486
1471.181191	4.838125	65.910490
1470.713815	9.928764	65.915495
1470.594113	4.641575	65.920500
1469.501289	2.174061	65.925505
1468.315204	11.926790	65.930510
1468.344423	-0.522818	65.935514
1467.579498	18.470001	65.940519
1467.244658	10.826381	65.945524
1466.002774	10.812605	65.950529
1465.569038	0.956510	65.955534
1465.424284	8.187799	65.960538
1464.058321	6.280932	65.965543
1463.509862	9.511069	65.970548
1462.753323	8.388843	65.975553
1461.795853	15.052308	65.980558
1461.257758	-0.509870	65.985562
1460.445430	12.785157	65.990567
1460.023147	6.084250	65.995572
1459.390832	9.165292	66.000577
1459.160340	11.636852	66.005582
1458.684704	4.479232	66.010586
1457.655599	12.975434	66.015591
1457.314252	4.676851	66.020596
1456.285695	4.291710	66.025601
1455.154421	10.604338	66.030606
1454.780602	2.487534	66.035610
1454.104171	9.767062	66.040615
1453.602157	9.090077	66.045620
1452.697004	3.602887	66.050625
1452.022624	7.170002	66.055630
1451.692395	6.249674	66.060634
1451.297575	14.452677	66.065639
1450.527598	4.003487	66.070644
1449.740506	7.703634	66.075649
1448.769636	3.154125	66.080654
1448.545806	3.005349	66.085658
1447.062406	8.628062	66.090663
1446.663202	7.978891	66.095668
1446.016360	2.135261	66.100673
1445.534462	8.877676	66.105678
1445.503233	4.856892	66.110682
1444.810858	8.436331	66.115687
1443.669909	4.106243	66.120692
1443.374744	7.800739	66.125697
1441.982424	10.784971	66.130702
1441.401803	-1.037851	66.135706
1440.399920	9.844648	66.140711
1439.935985	9.877538	66.145716
1439.843949	6.150267	66.150721
1439.102512	11.508395	66.155726
1439.055106	4.695868	66.160730
1437.416564	14.700297	66.165735
1437.099638	7.328223	66.170740
1436.825153	6.392729	66.175745
1435.887956	10.531471	66.180750
1434.930537	6.847139	66.185754
1434.536210	8.169930	66.190759
1434.051383	2.035628	66.195764
1432.449074	9.973254	66.200769
1431.944223	9.369263	66.205774
1432.025858	6.226235	66.210778
1431.288459	0.564159	66.215783
1430.866212	2.009658	66.220788
1430.301450	0.357073	66.225793
1429.148902	6.956937	66.230798
1428.430010	-1.283201	66.235802
1427.276231	9.688100	66.240807
1426.801737	7.171203	66.245812
1426.552124	15.116165	66.250817
1425.903744	15.468531	66.255822
1425.777356	-1.964657	66.260826
1424.428298	10.814882	66.265831
1423.963012	12.975264	66.270836
1423.822693	8.587051	66.275841
1422.481998	14.308518	66.280846
1421.725424	5.512983	66.285850
1421.121096	18.571536	66.290855
1420.704014	7.895952	66.295860
1419.933854	6.050518	66.300865
1418.870256	3.335534	66.305870
1418.519635	6.753424	66.310874
1417.835059	8.027739	66.315879
1417.345352	4.412568	66.320884
1416.205076	9.953947	66.325889
1415.676376	4.626124	66.330894
1415.550814	6.431312	66.335898
1414.949588	8.625920	66.340903
1413.839593	6.161160	66.345908
1413.222421	2.126290	66.350913
1412.383599	10.694757	66.355918
1412.085273	3.147849	66.360922
1411.198853	5.053483	66.365927
1410.463100	5.750896	66.370932
1410.033064	7.927754	66.375937
1409.515066	11.236636	66.380942
1409.143107	-1.369961	66.385946
1407.877561	8.578341	66.390951
1407.407349	12.702783	66.395956
1407.067591	2.806533	66.400961
1405.597461	2.021683	66.405966
1404.878712	5.539092	66.410970
1404.320839	11.598166	66.415975
1404.037045	11.217656	66.420980
1403.478958	4.579351	66.425985
1402.864992	8.784991	66.430990
1402.345368	-2.771550	66.435994
1401.384469	13.437610	66.440999
1400.950028	10.543773	66.446004
1399.791848	3.712285	66.451009
1399.296170	5.519540	66.456014
1398.784163	4.776347	66.461018
1398.617860	8.158631	66.466023
1397.769809	6.648855	66.471028
1396.705040	-1.476364	66.476033
1396.045947	3.532796	66.481038
1395.564620	5.328309	66.486042
1394.509740	6.437573	66.491047
1393.824351	9.121796	66.496052
1393.274184	7.295014	66.501057
1392.766277	6.576402	66.506062
1392.587526	-4.047167	66.511066
1391.108396	14.619227	66.516071
1390.474371	12.081967	66.521076
1390.390717	7.492365	66.526081
1390.065495	10.374796	66.531086
1389.285252	5.455968	66.536090
1388.012647	5.281536	66.541095
1387.367577	3.993382	66.546100
1387.392698	7.660621	66.551105
1385.823858	14.083835	66.556110
1385.483956	5.728269	66.561114
1385.052386	2.903365	66.566119
1384.508360	2.989997	66.571124
1383.475034	6.926422	66.576129
1382.532452	5.501064	66.581134
1382.399588	10.972191	66.586138
1381.949803	4.125867	66.591143
1380.653673	4.343103	66.596148
1379.865706	7.485175	66.601153
1379.471506	7.611068	66.606158
1379.193622	5.174887	66.611162
1378.164964	3.958754	66.616167
1377.250444	-1.471721	66.621172
1376.852690	-0.291877	66.626177
1376.195061	2.640244	66.631182
1375.980371	10.529190	66.636186
1375.044430	6.563929	66.641191
1374.368568	3.642248	66.646196
1373.973323	3.514422	66.651201
1372.832239	3.995590	66.656206
1371.696504	3.208060	66.661210
1371.046683	4.891594	66.666215
1370.621131	4.180393	66.671220
1370.418227	7.249957	66.676225
1369.874800	8.997001	66.681230
1369.678131	1.380325	66.686234
1368.637409	0.563500	66.691239
1368.059013	-1.134210	66.696244
1367.559475	-3.850535	66.701249
1366.153926	14.127670	66.706254
1365.716847	-0.725144	66.711258
1365.321828	0.082112	66.716263
1364.302103	4.713381	66.721268
1363.456033	-0.718509	66.726273
1362.868346	7.972466	66.731278
1362.820970	2.399406	66.736282
1362.123248	4.161519	66.741287
1360.697905	14.381248	66.746292
1360.372026	3.479877	66.751297
1359.653865	14.522295	66.756302
1359.371526	-3.428544	66.761306
1358.080944	9.787992	66.766311
1357.771275	-0.857336	66.771316
1357.260814	-2.471228	66.776321
1357.006722	-4.296186	66.781326
1356.135077	1.182005	66.786330
1355.010791	2.480512	66.791335
1354.476594	1.496433	66.796340
1354.207639	6.074577	66.801345
1353.099471	13.362841	66.806350
1352.332864	1.743079	66.811354
1351.737789	4.334106	66.816359
1351.225893	-4.372564	66.821364
1350.137471	7.140293	66.826369
1349.487131	7.902990	66.831374
1348.982530	2.418393	66.836378
1348.481415	7.777756	66.841383
1348.269880	18.391132	66.846388
1347.576365	-0.372684	66.851393
1346.344909	8.379643	66.856398
1345.980647	9.178859	66.861402
1345.344117	10.130170	66.866407
1344.601765	2.753215	66.871412
1343.656705	4.865310	66.876417
1343.455595	16.437375	66.881422
1343.073977	6.957794	66.886426
1342.163367	-3.424832	66.891431
1341.419849	12.073276	66.896436
1341.137076	2.279944	66.901441
1339.820676	16.426253	66.906446
1339.266037	8.678837	66.911450
1338.662666	10.284032	66.916455
1338.287884	9.689342	66.921460
1337.392207	2.771999	66.926465
1336.423520	10.993708	66.931470
1336.158099	-2.132845	66.936474
1335.521602	2.558927	66.941479
1334.310730	8.188830	66.946484
1334.016945	3.321988	66.951489
1332.949536	10.483931	66.956494
1333.028938	10.638609	66.961498
1332.396964	7.257384	66.966503
1331.311120	5.787016	66.971508
1330.793495	7.115233	66.976513
1329.972966	13.520426	66.981518
1329.521207	6.825813	66.986522
1328.171855	10.300003	66.991527
1327.661112	11.761165	66.996532
1327.655504	1.826000	67.001537
1327.035209	7.448738	67.006542
1326.451192	-4.069154	67.011546
1325.349775	10.686359	67.016551
1325.019209	1.435207	67.021556
1324.238676	-3.727971	67.026561
1322.856592	8.498625	67.031566
1322.662632	-9.318017	67.036570
1321.952102	7.816422	67.041575
1321.923005	1.852536	67.046580
1321.370292	6.177759	67.051585
1320.237727	4.326902	67.056590
1319.580023	-3.378884	67.061594
1318.828827	4.715208	67.066599
1317.814251	-4.138605	67.071604
1317.292471	5.423396	67.076609
1316.626460	10.323290	67.081614
1316.521646	0.667247	67.086618
1315.571892	6.462217	67.091623
1314.882306	8.036971	67.096628
1314.289282	7.144254	67.101633
1313.765357	6.335165	67.106638
1312.901237	-7.856801	67.111642
1312.290473	0.784231	67.116647
1311.351159	-7.335659	67.121652
1311.128057	-7.631192	67.126657
1310.317252	5.294612	67.131662
1309.505134	0.999037	67.136666
1308.769551	7.217264	67.141671
1308.304180	-2.923909	67.146676
1308.161574	3.152725	67.151681
1306.796507	3.477151	67.156686
1306.123666	-2.273991	67.161690
1305.395821	3.405274	67.166695
1305.115882	-1.887955	67.171700
1304.150856	-3.211943	67.176705
1303.312297	9.670970	67.181710
1303.207315	2.145381	67.186714
1302.736600	9.428496	67.191719
1301.963033	3.821099	67.196724
1300.859758	4.327826	67.201729
1300.402949	-0.768548	67.206734
1299.649674	6.912725	67.211738
1298.630150	5.152711	67.216743
1298.015145	-3.862396	67.221748
1297.935894	-0.776222	67.226753
1297.411256	8.887160	67.231758
1296.871978	6.022631	67.236762
1295.671320	4.125842	67.241767
1294.954266	2.838120	67.246772
1294.712670	-4.728819	67.251777
1293.311720	8.013288	67.256782
1293.070423	4.336570	67.261786
1292.269929	12.957318	67.266791
1291.863376	-1.294785	67.271796
1291.236867	7.785565	67.276801
1290.227585	9.816429	67.281806
1289.791141	5.530510	67.286810
1289.480208	3.856521	67.291815
1288.428878	5.151340	67.296820
1287.851780	12.533374	67.301825
1286.971545	8.130367	67.306830
1286.790471	5.582613	67.311834
1285.544427	5.642124	67.316839
1284.539640	7.744814	67.321844
1284.427198	-2.711086	67.326849
1283.772537	0.726776	67.331854
1283.973771	-0.282767	67.336858
1282.624242	9.712053	67.341863
1281.722111	8.784918	67.346868
1281.536252	-5.718309	67.351873
1280.057044	0.594513	67.356878
1279.723415	-3.848097	67.361882
1278.984573	0.729075	67.366887
1278.376242	5.908381	67.371892
1278.508095	3.402330	67.376897
1277.444226	4.607686	67.381902
1276.846848	5.596941	67.386906
1275.653167	-1.026987	67.391911
1275.204094	-2.221700	67.396916
1274.547541	-0.808304	67.401921
1273.436024	5.699939	67.406926
1273.161453	-5.148062	67.411930
1272.914872	-2.623473	67.416935
1272.215182	-5.249603	67.421940
1271.357716	-3.714374	67.426945
1270.397795	4.318302	67.431950
1270.307543	-2.553623	67.436954
1268.868476	5.717670	67.441959
1267.959874	-2.003394	67.446964
1267.695106	-4.135720	67.451969
1267.419585	6.304896	67.456974
1266.934321	0.489246	67.461978
1266.707075	-8.292623	67.466983
1265.537508	-9.175647	67.471988
1264.969408	1.450261	67.476993
1263.818930	6.372011	67.481998
1262.860505	4.160758	67.487002
1262.635879	4.434741	67.492007
1262.225891	4.818623	67.497012
1261.751701	5.800907	67.502017
1260.370918	10.182129	67.507022
1260.130407	2.304365	67.512026
1259.550782	5.017532	67.517031
1258.970758	3.999761	67.522036
1258.008719	0.499162	67.527041
1257.470483	2.486670	67.532046
1257.186835	-5.094076	67.537050
1255.958880	6.385805	67.542055
1255.406564	4.931552	67.547060
1254.996043	-0.041288	67.552065
1254.325211	1.462690	67.557070
1253.114516	-9.452477	67.562074
1252.424805	-0.398345	67.567079
1252.040591	3.119517	67.572084
1251.469798	1.797511	67.577089
1250.946087	-3.311866	67.582094
1250.038177	-9.421413	67.587098
1249.234589	-1.315825	67.592103
1248.917628	-1.773041	67.597108
1248.811251	2.175292	67.602113
1247.373667	1.103089	67.607118
1246.941880	-9.412401	67.612122
1246.459393	4.221278	67.617127
1245.577170	7.569184	67.622132
1244.779143	4.190738	67.627137
1243.784151	1.196846	67.632142
1244.096930	-5.937859	67.637146
1242.839604	3.126119	67.642151
1242.006113	2.694276	67.647156
1241.672742	-8.194827	67.652161
1240.829685	0.300232	67.657166
1240.110292	-5.686330	67.662170
1239.471285	-0.241948	67.667175
1238.705973	-1.085171	67.672180
1238.353532	-1.656590	67.677185
1237.590174	-1.733739	67.682190
1237.186102	-5.244215	67.687194
1236.035826	2.200589	67.692199
1235.371080	-1.039780	67.697204
1235.415463	-3.055689	67.702209
1234.353065	3.859487	67.707214
1233.600142	-1.461011	67.712218
1233.260846	-0.243136	67.717223
1232.390197	-7.486101	67.722228
1231.514979	-2.843078	67.727233
1230.351697	-5.980506	67.732238
1230.436101	-11.634430	67.737242
1229.727238	-0.654982	67.742247
1229.438480	2.073434	67.747252
1228.344413	-9.252920	67.752257
1227.575866	11.006754	67.757262
1227.205048	-5.047124	67.762266
1226.600358	3.633955	67.767271
1225.172859	7.458085	67.772276
1224.823797	-11.191708	67.777281
1224.508291	-7.572810	67.782286
1224.244864	-10.370804	67.787290
1223.250917	-4.191898	67.792295
1222.063141	-0.470547	67.797300
1222.031472	2.456675	67.802305
1221.390833	6.161976	67.807310
1220.070344	-0.277755	67.812314
1219.614269	-0.501536	67.817319
1219.112020	-0.151859	67.822324
1218.649842	-1.655131	67.827329
1217.950543	2.359114	67.832334
1217.136648	-0.275644	67.837338
1216.472177	7.978139	67.842343
1215.917935	-5.187602	67.847348
1215.000197	1.466458	67.852353
1214.195423	9.819826	67.857358
1214.022043	-3.620949	67.862362
1213.607789	9.642347	67.867367
1212.541811	11.704334	67.872372
1211.852256	2.240648	67.877377
1211.257374	4.216674	67.882382
1210.680377	-0.458450	67.887386
1209.695173	1.295807	67.892391
1209.082546	9.107693	67.897396
1208.876488	3.064729	67.902401
1207.444191	8.242630	67.907406
1206.998292	9.390733	67.912410
1206.400206	1.383771	67.917415
1205.933499	2.470529	67.922420
1205.562901	5.377539	67.927425
1204.533362	7.457388	67.932430
1204.026510	-7.436307	67.937434
1203.489954	12.149399	67.942439
1202.506755	4.127994	67.947444
1201.781748	6.952602	67.952449
1200.645294	15.582650	67.957454
1200.479359	7.615764	67.962458
1200.045600	5.270630	67.967463
1199.397876	10.574486	67.972468
1198.659475	-5.307382	67.977473
1198.224188	7.060411	67.982478
1197.823428	1.806915	67.987482
1196.886049	13.004069	67.992487
1196.057219	2.834001	67.997492
1195.825430	1.119053	68.002497
1194.583733	8.848069	68.007502
1193.668002	-2.189673	68.012506
1193.037719	3.988176	68.017511
1192.603811	5.001912	68.022516
1192.417599	7.332406	68.027521
1191.359685	4.857889	68.032526
1190.713677	-3.526211	68.037530
1190.184673	-4.599387	68.042535
1189.367239	-4.100229	68.047540
1188.427140	-9.133900	68.052545
1187.608536	-0.034026	68.057550
1187.344562	-6.230195	68.062554
1187.249272	-5.382277	68.067559
1185.829369	-0.061262	68.072564
1185.385685	-0.924084	68.077569
1184.569763	-0.814665	68.082574
1184.591975	-7.665042	68.087578
1183.862225	-1.846681	68.092583
1182.620593	-0.865321	68.097588
1181.892221	2.261018	68.102593
1181.473336	-0.852861	68.107598
1181.249687	-4.953407	68.112602
1179.873337	3.221221	68.117607
1179.603720	-1.835513	68.122612
1179.234329	-1.888575	68.127617
1178.072506	3.342513	68.132622
1177.175507	-5.561469	68.137626
1176.910999	0.230205	68.142631
1176.469855	2.995478	68.147636
1175.734581	-2.572230	68.152641
1174.645697	-3.758198	68.157646
1174.245156	-2.426498	68.162650
1173.671648	-7.814932	68.167655
1172.638903	-1.755991	68.172660
1172.051115	-0.361393	68.177665
1171.298878	-6.202360	68.182670
1171.023472	-4.319718	68.187674
1170.788155	-0.005531	68.192679
1169.348151	-2.990109	68.197684
1169.360103	0.128865	68.202689
1168.214451	-5.389335	68.207694
1167.560079	3.402155	68.212698
1166.806198	3.804481	68.217703
1166.250311	1.491395	68.222708
1166.147607	-8.079802	68.227713
1164.543730	3.825748	68.232718
1163.992720	-7.101257	68.237722
1163.672749	4.730964	68.242727
1163.160494	-6.077629	68.247732
1162.211759	-12.617451	68.252737
1161.313598	-1.642575	68.257742
1161.148426	-1.403271	68.262746
1160.615576	-3.906096	68.267751
1159.476142	1.081745	68.272756
1159.105072	-4.395655	68.277761
1157.947806	-2.095205	68.282766
1157.562710	-1.177536	68.287770
1157.153489	-7.673865	68.292775
1156.405306	12.049578	68.297780
1155.940837	-8.575067	68.302785
1155.421276	9.688049	68.307790
1154.451326	-4.878084	68.312794
1153.265634	0.300040	68.317799
1152.580759	8.971810	68.322804
1152.325746	-2.029084	68.327809
1152.175476	5.991535	68.332814
1151.452163	3.555275	68.337818
1150.348428	1.010796	68.342823
1149.295200	2.455780	68.347828
1149.343187	6.084677	68.352833
1148.364345	-2.992352	68.357838
1148.005546	0.228171	68.362842
1147.425166	-5.726855	68.367847
1146.327857	4.953284	68.372852
1145.661061	-13.097169	68.377857
1144.910937	4.707462	68.382862
1144.719300	-11.890536	68.387866
1144.199173	-3.233939	68.392871
1143.153347	0.070637	68.397876
1142.602322	4.777236	68.402881
1141.553179	2.599385	68.407886
1141.639897	-1.066410	68.412890
1140.238103	-3.274896	68.417895
1139.511265	6.535780	68.422900
1139.198631	1.763432	68.427905
1138.550734	9.000632	68.432910
1137.904344	-1.520120	68.437914
1137.238881	3.859106	68.442919
1136.633168	7.874254	68.447924
1136.344815	2.235468	68.452929
1135.139756	2.939802	68.457934
1134.476123	2.469937	68.462938
1133.558852	4.284377	68.467943
1133.178586	5.417320	68.472948
1132.788307	1.909400	68.477953
1131.775202	7.157851	68.482958
1131.400865	4.886855	68.487962
1130.922628	-4.033258	68.492967
1129.887887	6.155973	68.497972
1129.476518	-5.007696	68.502977
1128.517029	16.245865	68.507982
1127.871984	2.520594	68.512986
1126.885057	-0.882953	68.517991
1126.334561	-1.213121	68.522996
1126.195706	-4.254842	68.528001
1125.630193	5.790365	68.533006
1124.795425	2.799421	68.538010
1123.897409	14.540678	68.543015
1123.252916	-1.844943	68.548020
1123.134588	3.021483	68.553025
1122.205294	6.451030	68.558030
1121.528267	0.987613	68.563034
1120.705138	7.639268	68.568039
1120.130396	-3.586718	68.573044
1119.032409	-3.932292	68.578049
1118.329557	8.708299	68.583054
1118.244679	-4.908955	68.588058
1117.619286	1.192437	68.593063
1116.571054	14.020436	68.598068
1115.883203	-7.811273	68.603073
1115.378195	-2.706724	68.608078
1115.074004	2.719113	68.613082
1114.013085	1.989184	68.618087
1113.219747	0.095499	68.623092
1112.822458	6.676260	68.628097
1112.133370	3.463454	68.633102
1111.692235	-9.567276	68.638106
1110.531480	-1.994608	68.643111
1109.844218	-10.433614	68.648116
1109.718967	-3.107671	68.653121
1108.950402	3.931112	68.658126
1108.001488	0.089450	68.663130
1107.272477	-4.503116	68.668135
1106.815296	6.803743	68.673140
1106.609858	-11.703279	68.678145
1105.597149	-1.191128	68.683150
1104.746999	-3.596156	68.688154
1104.546399	-5.904245	68.693159
1103.250790	3.044455	68.698164
1102.684729	-6.984444	68.703169
1101.713729	-7.008019	68.708174
1101.536803	-8.657568	68.713178
1101.458658	-3.983614	68.718183
1100.699194	1.096765	68.723188
1099.833635	-2.056424	68.728193
1098.946249	1.872654	68.733198
1097.548550	-10.212707	68.738202
1097.278291	-5.382038	68.743207
1096.857624	-0.448594	68.748212
1096.484041	-1.860281	68.753217
1095.641128	0.331842	68.758222
1095.343797	2.238480	68.763226
1094.387103	-2.671091	68.768231
1093.833652	0.436904	68.773236
1093.033630	5.135817	68.778241
1091.619475	1.363442	68.783246
1091.354437	-7.268882	68.788250
1091.371329	0.733024	68.793255
1090.376305	-0.526185	68.798260
1089.342579	-8.126338	68.803265
1088.604855	-11.124819	68.808270
1088.438835	2.912671	68.813274
1088.150369	0.076100	68.818279
1087.146409	1.869655	68.823284
1086.402520	-10.338634	68.828289
1085.627318	-1.712411	68.833294
1085.258797	-2.700711	68.838298
1084.617273	0.216298	68.843303
1084.126693	7.155673	68.848308
1083.274470	-0.571125	68.853313
1082.074982	-0.173575	68.858318
1081.672040	-0.364784	68.863322
1081.381150	1.113485	68.868327
1080.546353	-2.662743	68.873332
1079.648286	2.783460	68.878337
1078.836502	-7.993221	68.883342
1078.283327	2.218756	68.888346
1078.121690	-0.268991	68.893351
1077.102050	8.683127	68.898356
1076.511389	1.433525	68.903361
1075.588966	-0.737649	68.908366
1075.170123	0.912361	68.913370
1074.588182	4.602047	68.918375
1073.532681	2.325891	68.923380
1072.812058	-5.412375	68.928385
1072.578522	-2.306388	68.933390
1071.949959	-0.370705	68.938394
1070.924404	-1.573010	68.943399
1070.589974	-8.357179	68.948404
1070.329409	-2.662321	68.953409
1069.141653	-0.063674	68.958414
1068.241854	-4.875054	68.963418
1067.931570	-6.151730	68.968423
1067.302940	0.867952	68.973428
1066.716234	-3.644740	68.978433
1065.647740	-4.088020	68.983438
1065.220098	-20.621633	68.988442
1064.845189	-3.800772	68.993447
1063.927333	-2.870868	68.998452
1063.236647	-3.289102	69.003457
1062.430961	-3.972885	69.008462
1062.135786	-6.461461	69.013466
1061.055614	-3.389506	69.018471
1060.012295	-3.543483	69.023476
1060.004737	-14.817101	69.028481
1059.458091	-4.481588	69.033486
1058.750363	-13.079740	69.038490
1058.000441	-6.010801	69.043495
1057.281848	0.627390	69.048500
1056.885392	-20.418017	69.053505
1055.896757	-4.986548	69.058510
1054.899949	4.274171	69.063514
1054.564730	-14.248453	69.068519
1053.739332	-0.457714	69.073524
1053.538415	-7.740927	69.078529
1052.710631	-5.177469	69.083534
1051.989222	-1.036669	69.088538
1051.399553	-0.341898	69.093543
1050.718393	0.372161	69.098548
1050.400657	-13.684254	69.103553
1049.176112	1.601835	69.108558
1048.446106	-4.099126	69.113562
1048.489996	-9.787599	69.118567
1047.237477	-2.829498	69.123572
1046.457439	-11.911294	69.128577
1045.879092	6.317017	69.133582
1045.644440	-7.998620	69.138586
1045.103380	-8.516347	69.143591
1043.916167	-2.077979	69.148596
1043.650959	-15.877824	69.153601
1042.938965	5.624931	69.158606
1041.962003	3.520793	69.163610
1041.516000	-8.589797	69.168615
1040.963168	3.803009	69.173620
1040.485441	-8.496494	69.178625
1039.520916	-4.668665	69.183630
1038.620275	-4.815372	69.188634
1038.295189	-8.928142	69.193639
1037.264706	0.194438	69.198644
1036.437770	-5.183597	69.203649
1035.821636	-0.173315	69.208654
1035.353839	-3.361382	69.213658
1035.191700	-3.154091	69.218663
1034.306825	-3.632881	69.223668
1033.610226	-10.952337	69.228673
1032.911891	-8.828931	69.233678
1032.293593	-9.796403	69.238682
1031.563199	-6.729628	69.243687
1030.838852	-5.393695	69.248692
1030.783264	0.427821	69.253697
1029.423243	7.179116	69.258702
1028.652282	0.585832	69.263706
1028.259553	-6.797743	69.268711
1027.526322	-0.018449	69.273716
1027.552854	-10.967913	69.278721
1026.089301	2.979564	69.283726
1025.581701	-6.667535	69.288730
1025.100436	-4.862509	69.293735
1023.982163	-8.579419	69.298740
1023.226621	0.486804	69.303745
1022.351353	2.274099	69.308750
1022.217819	-3.099145	69.313754
1021.923940	-2.468777	69.318759
1021.345774	2.029276	69.323764
1020.714610	-2.255561	69.328769
1019.931784	-2.550315	69.333774
1018.852751	-6.886887	69.338778
1018.085214	-12.391055	69.343783
1017.382437	-2.180502	69.348788
1017.146266	-2.980119	69.353793
1016.730969	-8.906180	69.358798
1015.860144	-8.840008	69.363802
1015.160469	-11.354099	69.368807
1014.270893	-8.843875	69.373812
1013.625324	-11.049614	69.378817
1012.529433	-12.655431	69.383822
1012.014101	-8.034916	69.388826
1011.491182	-3.668653	69.393831
1011.131618	-10.500847	69.398836
1011.099205	-9.468968	69.403841
1009.739719	-1.377372	69.408846
1009.283651	-7.971866	69.413850
1008.836394	-14.305990	69.418855
1007.354664	1.501994	69.423860
1007.262624	-3.620813	69.428865
1006.343660	-7.229082	69.433870
1006.109902	-7.327354	69.438874
1005.112217	-19.695484	69.443879
1004.255769	-4.803843	69.448884
1003.872242	-9.320461	69.453889
1002.976926	-6.042937	69.458894
1002.044108	-7.792967	69.463898
1001.514264	-7.104550	69.468903
1001.362423	-5.738284	69.473908
1001.117267	-8.346771	69.478913
999.634458	-0.054202	69.483918
999.308683	-6.074928	69.488922
999.061496	-4.982065	69.493927
997.981804	2.445287	69.498932
997.355053	-4.648736	69.503937
996.585244	2.133233	69.508942
995.644083	-7.938442	69.513946
994.478561	-0.934238	69.518951
993.817818	-2.271830	69.523956
993.669679	-7.738938	69.528961
993.487906	-4.303723	69.533966
992.971482	3.316271	69.538970
992.499223	-8.350166	69.543975
991.288600	-7.192304	69.548980
991.003147	-1.909789	69.553985
990.018261	1.752570	69.558990
989.146527	-2.110786	69.563994
988.927953	0.806750	69.568999
987.784563	5.908828	69.574004
986.972620	-6.884667	69.579009
986.264538	-1.383516	69.584014
985.903987	-3.525795	69.589018
985.686012	0.966986	69.594023
984.817966	0.834035	69.599028
984.024753	-7.531298	69.604033
983.291542	-1.042150	69.609038
982.736832	-7.715555	69.614042
981.789944	-6.490849	69.619047
981.003715	3.037573	69.624052
980.727637	-2.141100	69.629057
980.441208	-1.530836	69.634062
979.225320	-7.077185	69.639066
978.379712	-2.799912	69.644071
977.983047	1.569921	69.649076
977.676473	-13.672515	69.654081
976.734336	-1.659295	69.659086
975.763351	-8.387878	69.664090
975.300761	-3.690595	69.669095
975.040565	-6.941646	69.674100
974.412773	-8.587244	69.679105
973.142713	1.237364	69.684110
972.692491	1.432156	69.689114
972.560596	-5.109839	69.694119
971.399830	8.592368	69.699124
970.621401	-4.119724	69.704129
970.351698	-0.990629	69.709134
969.894240	-0.949223	69.714138
968.710017	-9.802669	69.719143
967.758821	-0.047726	69.724148
967.560435	-13.443458	69.729153
966.845117	-5.484316	69.734158
965.756371	-4.358452	69.739162
965.301456	-5.673598	69.744167
964.223478	-5.385214	69.749172
964.757889	-4.210153	69.754177
963.926390	-3.860069	69.759182
962.700621	-1.630632	69.764186
962.422398	-8.448953	69.769191
961.717997	5.272091	69.774196
961.045375	-8.746751	69.779201
959.888758	1.909768	69.784206
959.702734	-7.935138	69.789210
959.258967	-1.375355	69.794215
957.538954	5.261377	69.799220
957.347769	-8.507656	69.804225
956.775216	-3.444373	69.809230
956.520347	0.128630	69.814234
955.940313	-8.820960	69.819239
954.822739	1.487156	69.824244
954.579512	-8.862721	69.829249
953.700259	-4.699933	69.834254
952.428889	6.782235	69.839258
951.952050	0.416557	69.844263
951.122325	-5.512922	69.849268
951.353006	-7.351901	69.854273
950.615281	-6.124201	69.859278
949.737751	1.649456	69.864282
949.270233	-12.641709	69.869287
948.345967	1.033899	69.874292
947.279320	-5.748832	69.879297
946.379614	5.978534	69.884302
946.029809	3.173822	69.889306
945.978357	-5.877232	69.894311
945.367562	4.026970	69.899316
945.093441	-12.043774	69.904321
943.867663	4.057812	69.909326
942.808926	2.655842	69.914330
941.960460	3.566862	69.919335
940.974764	1.572963	69.924340
940.856751	-6.169695	69.929345
940.685531	6.113505	69.934350
940.065405	4.840425	69.939354
939.462030	1.686570	69.944359
938.402425	1.032198	69.949364
938.101954	-7.241226	69.954369
936.711644	-4.518825	69.959374
935.945238	5.662451	69.964378
935.617417	-1.969549	69.969383
935.153548	12.290377	69.974388
935.003075	-9.943719	69.979393
933.579818	1.942662	69.984398
932.728028	5.505013	69.989402
932.358241	-3.446494	69.994407
931.932410	-2.908655	69.999412
931.591466	-11.044750	70.004417
930.157581	4.016080	70.009422
929.722717	-4.005726	70.014426
929.540860	-0.315034	70.019431
928.223283	1.766607	70.024436
927.690464	-8.057792	70.029441
926.996173	-0.113025	70.034446
926.889041	-2.685125	70.039450
926.159021	4.379105	70.044455
925.057054	-0.554580	70.049460
924.918018	-7.950121	70.054465
924.070740	-3.724606	70.059470
922.992033	2.491544	70.064474
922.926434	-5.511760	70.069479
921.956825	3.568055	70.074484
921.221077	-7.231697	70.079489
920.577700	-0.958678	70.084494
919.825998	0.061525	70.089498
919.585804	0.051017	70.094503
918.478029	2.761577	70.099508
917.654371	2.787161	70.104513
917.055877	-1.428730	70.109518
916.568049	1.009703	70.114522
916.147800	-8.070958	70.119527
915.108580	-9.663674	70.124532
914.576154	-3.313699	70.129537
914.302044	-11.266467	70.134542
913.350139	4.461965	70.139546
912.894402	-5.849351	70.144551
911.941228	-1.782015	70.149556
911.489379	-4.378095	70.154561
910.516854	-4.355624	70.159566
909.837491	2.738391	70.164570
909.665186	-11.713284	70.169575
908.704701	2.228290	70.174580
907.785820	-6.058665	70.179585
906.860793	4.248784	70.184590
906.278679	-11.731929	70.189594
906.245574	-8.995294	70.194599
905.808764	-1.588232	70.199604
905.074018	-6.354853	70.204609
904.036636	-5.040023	70.209614
903.635234	1.888330	70.214618
903.022861	-4.075724	70.219623
901.511662	3.723109	70.224628
901.231455	-14.730949	70.229633
900.790667	1.818129	70.234638
900.232483	-8.349147	70.239642
899.296678	-3.887189	70.244647
898.454049	0.336018	70.249652
898.334766	-2.331914	70.254657
897.769278	1.672145	70.259662
896.661619	-4.176807	70.264666
896.157919	-7.247167	70.269671
895.378659	1.119552	70.274676
894.914996	-10.068837	70.279681
894.048927	7.459393	70.284686
893.249599	0.514292	70.289690
893.218743	-5.715776	70.294695
892.267255	-1.520971	70.299700
891.405903	-6.567050	70.304705
890.589886	-11.069999	70.309710
890.004744	-1.959912	70.314714
889.944410	-3.697384	70.319719
888.992326	1.434206	70.324724
888.476822	-4.723454	70.329729
887.804514	-4.444413	70.334734
886.614774	-10.029564	70.339738
886.000414	-4.213734	70.344743
885.407521	-1.252383	70.349748
885.326753	-17.760723	70.354753
883.970062	4.678841	70.359758
882.985449	-5.732786	70.364762
882.327855	-7.312116	70.369767
881.938490	-3.074320	70.374772
881.950826	-9.230838	70.379777
881.287098	-9.542928	70.384782
880.752577	-5.381373	70.389786
879.810276	-5.087741	70.394791
879.169450	1.323649	70.399796
878.436659	-5.567380	70.404801
877.476489	-0.421885	70.409806
876.836066	-0.168417	70.414810
876.770044	-11.199324	70.419815
875.519770	-7.113072	70.424820
874.949094	-12.408832	70.429825
874.620997	-14.450603	70.434830
873.797517	-11.201820	70.439834
872.998508	-14.740819	70.444839
872.249413	-8.619697	70.449844
872.165278	-10.742877	70.454849
870.994212	-7.336266	70.459854
870.184377	-2.481198	70.464858
869.816974	-3.658871	70.469863
869.158459	-8.070191	70.474868
868.349190	-9.617489	70.479873
867.653974	-9.702219	70.484878
867.251337	-5.066503	70.489882
866.624280	-15.102954	70.494887
865.375611	-5.273829	70.499892
864.880776	-6.768677	70.504897
864.327670	-4.628921	70.509902
864.053527	-11.140373	70.514906
863.407578	-3.652711	70.519911
862.453155	-1.493227	70.524916
861.714847	-6.065305	70.529921
861.380035	3.350287	70.534926
860.114926	-6.329144	70.539930
859.421411	1.577668	70.544935
858.551261	2.146822	70.549940
858.953291	-3.112962	70.554945
858.268912	-10.893183	70.559950
857.107835	2.894257	70.564954
856.448222	-7.793010	70.569959
856.102879	-7.118163	70.574964
855.429192	-3.270335	70.579969
854.450246	-4.650274	70.584974
853.637155	0.344086	70.589978
853.628149	-9.316093	70.594983
852.445301	1.062369	70.599988
851.560545	-7.680990	70.604993
851.057241	-8.007569	70.609998
850.254232	1.514088	70.615002
850.438156	-11.297517	70.620007
848.900317	0.676523	70.625012
848.271401	2.855158	70.630017
847.968549	3.439666	70.635022
847.401663	-0.625121	70.640026
846.755611	-7.689213	70.645031
845.890678	-12.430357	70.650036
845.627302	-5.539743	70.655041
844.678895	-0.566417	70.660046
844.118994	-1.599906	70.665050
843.566249	-5.439866	70.670055
842.460082	3.188634	70.675060
841.741161	-7.115458	70.680065
841.052290	-1.778178	70.685070
840.791941	-6.256025	70.690074
840.490594	-13.486945	70.695079
839.311095	1.257464	70.700084
838.014952	-9.894581	70.705089
837.836327	-8.445198	70.710094
837.551549	-0.612910	70.715098
837.381012	-2.768065	70.720103
835.978618	-3.033519	70.725108
835.398520	-5.536629	70.730113
834.978940	-3.504853	70.735118
833.740664	2.137502	70.740122
833.374884	-14.322306	70.745127
832.852062	4.523205	70.750132
832.556408	-10.687815	70.755137
831.604016	-4.480704	70.760142
830.485827	-2.820253	70.765146
830.474605	-10.354394	70.770151
829.336500	-10.627223	70.775156
828.835633	-0.311588	70.780161
827.884841	-2.667379	70.785166
827.387975	-2.113483	70.790170
826.538524	-7.265506	70.795175
825.498037	-4.660235	70.800180
825.215456	2.353286	70.805185
824.866106	-1.899085	70.810190
824.611560	-4.003020	70.815194
824.204946	-10.446069	70.820199
822.911789	-3.044600	70.825204
822.144788	1.590781	70.830209
821.108707	-12.313369	70.835214
819.979350	-5.955085	70.840218
820.047680	-4.294284	70.845223
819.333044	2.565672	70.850228
819.323986	-4.539895	70.855233
818.655224	2.005261	70.860238
817.685614	-3.851436	70.865242
817.022228	-0.497236	70.870247
816.466936	-1.544067	70.875252
815.089838	-3.981794	70.880257
814.361711	2.356776	70.885262
813.943247	-3.381083	70.890266
814.037003	2.989069	70.895271
812.906777	10.754110	70.900276
812.133422	-0.840687	70.905281
811.748682	1.633390	70.910286
810.972756	2.591251	70.915290
810.655150	-1.521095	70.920295
809.358631	3.756815	70.925300
809.000223	3.408753	70.930305
808.416196	-4.701235	70.935310
807.484729	0.941172	70.940314
806.981729	-5.156956	70.945319
806.159306	0.819745	70.950324
805.838543	-5.905045	70.955329
804.699639	-0.947110	70.960334
803.892386	0.594468	70.965338
803.581432	-2.454518	70.970343
803.040828	1.504597	70.975348
802.876529	-11.270490	70.980353
802.108529	-2.479778	70.985358
801.183039	6.525241	70.990362
800.650925	-2.365700	70.995367
799.359048	-2.740188	71.000372
798.693016	-6.358678	71.005377
798.510888	4.182179	71.010382
798.000370	-2.826207	71.015386
796.931602	-7.684689	71.020391
796.061188	-1.782347	71.025396
795.625177	4.329954	71.030401
795.320994	-0.301755	71.035406
794.558963	-2.960390	71.040410
793.979680	-9.516288	71.045415
792.914874	-7.977858	71.050420
792.747324	-7.161001	71.055425
791.629432	-11.639507	71.060430
790.743469	-0.655447	71.065434
790.328092	-12.193680	71.070439
789.704621	3.763179	71.075444
789.301192	-3.640714	71.080449
788.681804	-4.980102	71.085454
787.902279	0.396854	71.090458
787.499294	-6.436265	71.095463
786.521766	0.044516	71.100468
785.997431	-8.191658	71.105473
785.149332	-10.056014	71.110478
784.270904	-7.954333	71.115482
783.552045	-1.822232	71.120487
782.599558	0.108319	71.125492
782.755571	-5.129651	71.130497
782.185389	-6.871099	71.135502
781.279448	2.362617	71.140506
780.648072	-7.930157	71.145511
779.548674	0.481249	71.150516
779.533129	-11.609482	71.155521
778.750107	-0.854693	71.160526
777.729509	-9.302006	71.165530
777.455227	-3.597068	71.170535
776.717413	-2.038153	71.175540
775.822794	-16.078333	71.180545
775.198437	-6.089957	71.185550
774.445830	-8.034166	71.190554
774.477418	-6.318634	71.195559
773.294105	-12.718433	71.200564
772.553295	-5.349691	71.205569
772.253757	-9.529558	71.210574
770.846653	-11.514637	71.215578
770.365182	-3.092806	71.220583
769.593587	-4.631877	71.225588
769.228391	-10.589510	71.230593
769.305503	-9.925144	71.235598
768.190911	-1.818815	71.240602
767.445813	-12.610702	71.245607
767.176504	-3.295424	71.250612
766.333327	1.147099	71.255617
765.222379	-4.876300	71.260622
764.727152	2.190003	71.265626
764.231695	-10.153893	71.270631
762.817018	-0.537984	71.275636
762.404292	-6.079630	71.280641
762.224538	-0.299857	71.285646
761.406486	-1.770029	71.290650
761.034786	-5.249295	71.295655
759.756338	-3.169069	71.300660
759.362262	-9.785983	71.305665
758.938823	-11.429367	71.310670
758.144845	-6.124220	71.315674
757.168824	0.864096	71.320679
756.311164	-3.528098	71.325684
756.240187	-5.718020	71.330689
755.951872	-9.557482	71.335694
754.890305	-7.533862	71.340698
754.301621	-10.699464	71.345703
753.656947	-6.824695	71.350708
752.908778	-12.841192	71.355713
751.848707	-16.751732	71.360718
751.235621	-5.150388	71.365722
751.071272	-16.514115	71.370727
750.273568	-9.197810	71.375732
749.258352	-6.949762	71.380737
748.595819	-19.197659	71.385742
748.160010	-15.630529	71.390746
747.961569	-12.378729	71.395751
746.822277	-7.330827	71.400756
746.211102	-9.705966	71.405761
745.991230	-11.022224	71.410766
744.410975	-9.546778	71.415770
743.874163	-18.384905	71.420775
743.143753	-1.835449	71.425780
742.815414	-9.197668	71.430785
742.604012	-10.991502	71.435790
741.708818	-7.762799	71.440794
741.141933	-5.592440	71.445799
740.400303	-1.654921	71.450804
739.707284	-8.391385	71.455809
738.582093	-11.022137	71.460814
737.725713	-9.764446	71.465818
737.784576	-12.344038	71.470823
737.169843	-9.265644	71.475828
736.556482	-4.556938	71.480833
735.629108	-3.133405	71.485838
735.162746	-2.598540	71.490842
734.958695	-10.573467	71.495847
733.441059	-2.535411	71.500852
732.936310	-4.326689	71.505857
732.333836	-6.206482	71.510862
730.862511	-1.621354	71.515866
730.649165	-4.144989	71.520871
730.170590	-9.772332	71.525876
729.939829	-8.131720	71.530881
729.662571	-2.710150	71.535886
728.680725	-7.574555	71.540890
728.172962	-4.771804	71.545895
727.366501	-11.144855	71.550900
726.020865	-3.080568	71.555905
725.725572	-2.421558	71.560910
724.900679	3.104561	71.565914
724.827829	-11.036487	71.570919
723.621041	-8.366851	71.575924
722.717443	-5.794376	71.580929
722.424954	-6.905108	71.585934
721.971352	-3.410831	71.590938
721.068637	-9.568285	71.595943
720.209520	-3.995719	71.600948
719.914552	-8.748725	71.605953
719.191961	-12.493798	71.610958
717.744605	-3.266895	71.615962
717.434238	-13.074607	71.620967
716.660136	-15.292910	71.625972
716.550702	-8.563997	71.630977
716.199386	-13.110915	71.635982
715.550688	-4.097915	71.640986
714.855258	-19.331963	71.645991
713.858836	-4.416405	71.650996
713.094733	-9.410090	71.656001
712.417064	-12.031668	71.661006
711.727186	-12.197626	71.666010
711.705602	-13.884490	71.671015
710.626161	-6.471274	71.676020
709.758886	-11.893217	71.681025
709.513773	-14.377097	71.686030
708.671754	-9.909514	71.691034
707.828729	-7.613177	71.696039
706.760011	-2.822494	71.701044
706.266967	-7.383112	71.706049
706.340366	-22.132469	71.711054
705.262958	-4.155843	71.716058
704.616761	-14.900375	71.721063
704.119400	-11.673511	71.726068
703.622526	-7.946843	71.731073
702.584808	-19.214060	71.736078
701.716676	-10.913575	71.741082
701.680516	-17.671044	71.746087
700.721556	-13.697333	71.751092
699.838047	-17.877232	71.756097
699.016444	-8.455087	71.761102
698.517480	-15.112051	71.766106
698.261613	-11.146224	71.771111
696.989876	-18.331393	71.776116
696.317901	-12.176783	71.781121
695.976047	-14.932253	71.786126
695.242589	-20.531610	71.791130
695.148773	-11.518666	71.796135
693.796129	-8.396870	71.801140
692.950586	-10.785134	71.806145
692.972515	-21.617128	71.811150
692.026042	-6.846713	71.816154
691.153616	-24.030007	71.821159
690.166679	-7.176357	71.826164
689.948139	-15.308234	71.831169
689.833045	-23.421887	71.836174
688.876997	-6.453310	71.841178
687.980581	-13.176286	71.846183
687.312566	-16.655656	71.851188
687.077969	-12.794139	71.856193
686.675458	-24.820069	71.861198
685.290093	-9.017847	71.866202
684.783375	-11.253489	71.871207
684.507892	-10.851512	71.876212
683.626264	-7.845718	71.881217
682.948257	-14.666549	71.886222
682.009732	-8.130450	71.891226
681.484072	-13.736089	71.896231
680.307804	-14.758113	71.901236
679.845658	-6.744618	71.906241
679.951087	-15.738617	71.911246
678.983203	-15.289452	71.916250
678.455065	-13.420134	71.921255
677.448085	-6.786402	71.926260
677.090826	-14.514574	71.931265
675.953271	-16.129371	71.936270
675.127010	-4.367917	71.941274
675.053053	-15.550487	71.946279
674.353356	-12.890623	71.951284
673.663987	-7.360846	71.956289
672.908796	-10.700177	71.961294
672.394449	-9.944777	71.966298
671.908254	-9.881393	71.971303
670.561149	-16.031130	71.976308
669.673118	-15.526870	71.981313
669.552018	-16.980271	71.986318
668.897842	-7.969548	71.991322
668.660117	-12.895659	71.996327
667.350714	-13.182134	72.001332
666.827233	-4.725218	72.006337
666.699460	-14.576188	72.011342
665.786115	-13.933859	72.016346
665.104050	-10.767458	72.021351
664.125043	-0.706813	72.026356
663.710479	-4.236004	72.031361
662.748854	-5.688008	72.036366
662.201773	-2.169373	72.041370
662.136857	-15.933209	72.046375
661.399323	-10.138724	72.051380
660.087677	-16.792404	72.056385
659.612029	-14.131949	72.061390
658.879675	-6.293033	72.066394
658.896406	-21.596317	72.071399
657.274651	-6.287853	72.076404
656.670071	-16.802456	72.081409
656.446418	-8.464253	72.086414
655.892188	-8.883604	72.091418
655.299244	-14.808095	72.096423
654.477589	-11.067541	72.101428
654.020661	-7.124882	72.106433
653.048731	-7.665363	72.111438
651.731327	-5.471650	72.116442
651.645443	-4.730868	72.121447
651.043999	-6.385305	72.126452
650.750145	-5.190366	72.131457
649.913126	-8.977116	72.136462
649.040032	-6.218668	72.141466
648.816607	-9.313106	72.146471
647.790680	-5.718207	72.151476
647.004164	-8.260931	72.156481
646.501812	-4.553881	72.161486
646.073904	-0.120690	72.166490
645.234457	-6.352843	72.171495
643.970825	-5.314105	72.176500
643.562736	-1.284607	72.181505
643.291058	-7.753836	72.186510
642.469516	3.328808	72.191514
642.047140	-9.236415	72.196519
641.092754	-4.146958	72.201524
640.744755	-12.184094	72.206529
640.059761	-14.258872	72.211534
638.809545	-6.329590	72.216538
638.717173	-14.252901	72.221543
637.950593	2.430062	72.226548
637.394201	-1.999029	72.231553
636.462220	-12.300639	72.236558
635.742715	-5.234874	72.241562
635.344647	-7.713307	72.246567
634.706673	-3.259275	72.251572
633.620823	-17.281539	72.256577
633.368064	-12.903054	72.261582
633.065057	-7.650841	72.266586
632.307671	3.785854	72.271591
631.045624	-2.326950	72.276596
630.803401	-7.736452	72.281601
629.831500	7.971573	72.286606
628.588338	2.890215	72.291610
628.062253	-1.753430	72.296615
627.595005	-10.414952	72.301620
627.306448	-17.166906	72.306625
627.280670	-7.541920	72.311630
626.454818	-8.287001	72.316634
625.994237	-18.405068	72.321639
624.594229	-4.150588	72.326644
623.675973	-10.437986	72.331649
623.289880	-5.098423	72.336654
622.485346	-1.097240	72.341658
622.495116	-2.153602	72.346663
621.423248	2.268619	72.351668
620.581531	-0.290536	72.356673
620.198025	-7.494136	72.361678
619.480821	-3.782822	72.366682
618.731263	-15.192084	72.371687
617.931415	2.723016	72.376692
617.580769	-3.678440	72.381697
617.079837	4.211937	72.386702
615.373644	6.352480	72.391706
615.182162	-12.979769	72.396711
614.572711	-3.488893	72.401716
614.075634	-6.356819	72.406721
614.029421	-10.174896	72.411726
612.440768	-4.730523	72.416730
612.293084	-10.235502	72.421735
611.513193	0.936704	72.426740
610.759597	-7.988281	72.431745
610.264499	-7.664854	72.436750
609.399219	-6.487702	72.441754
609.020477	-2.357221	72.446759
608.256191	-7.399724	72.451764
607.349241	-4.743099	72.456769
606.852569	-3.249353	72.461774
606.192745	-1.256546	72.466778
605.630535	-12.706683	72.471783
604.879130	3.470833	72.476788
604.475658	-9.184120	72.481793
603.439164	-8.802843	72.486798
602.289130	-5.364774	72.491802
602.007916	-18.225267	72.496807
601.604468	-3.766820	72.501812
601.462324	-9.012490	72.506817
600.280539	-17.880301	72.511822
599.336754	-1.268457	72.516826
599.216093	-14.392640	72.521831
598.467207	-4.444326	72.526836
597.387954	-11.978634	72.531841
596.514718	-7.255316	72.536846
596.211296	-9.882855	72.541850
595.850306	-17.793333	72.546855
594.999344	-3.632602	72.551860
594.155757	-4.340155	72.556865
593.583606	-19.150673	72.561870
593.265405	-5.543145	72.566874
592.373721	-13.529939	72.571879
591.559169	-19.969450	72.576884
590.966311	-2.155130	72.581889
590.600572	-17.648214	72.586894
589.652637	-10.680093	72.591898
589.027451	-8.006845	72.596903
588.649173	-0.791998	72.601908
587.679572	-5.377600	72.606913
586.474050	-6.462727	72.611918
585.737597	-11.545921	72.616922
585.511130	-8.636570	72.621927
585.299341	-8.232113	72.626932
584.545163	-3.715407	72.631937
583.926252	-10.514080	72.636942
582.941611	-7.058195	72.641946
582.647167	-5.976692	72.646951
581.552760	-13.787690	72.651956
580.619266	-3.937696	72.656961
580.470747	-11.823672	72.661966
579.792124	-7.049350	72.666970
579.632553	-9.286650	72.671975
578.728674	-2.357078	72.676980
577.917205	-5.941295	72.681985
577.488364	-13.330044	72.686990
576.272624	1.205759	72.691994
575.692336	-3.624774	72.696999
575.076641	-2.900517	72.702004
574.381943	-3.327437	72.707009
573.898929	-0.145411	72.712014
573.335218	4.452921	72.717018
572.933901	-16.252491	72.722023
571.889662	-3.765607	72.727028
570.962461	-10.748550	72.732033
570.479206	-13.349015	72.737038
569.998644	-8.927931	72.742042
569.347730	-15.227926	72.747047
568.130477	-4.454390	72.752052
567.570987	-2.515402	72.757057
567.577620	-9.921481	72.762062
566.262415	-1.157090	72.767066
565.577676	-11.669933	72.772071
564.889116	-5.290307	72.777076
564.771451	-14.270839	72.782081
564.555754	-12.826574	72.787086
562.946143	-5.570120	72.792090
562.283481	-3.881194	72.797095
562.103913	-5.383621	72.802100
561.478755	-7.489985	72.807105
560.532618	-10.333672	72.812110
559.650750	-6.966688	72.817114
559.404429	-7.200106	72.822119
559.044659	-3.241372	72.827124
557.868606	-7.894995	72.832129
557.415847	-15.937500	72.837134
556.598782	-9.613094	72.842138
556.022930	-12.403804	72.847143
555.151854	-4.380346	72.852148
554.533244	0.903228	72.857153
554.502039	-20.690584	72.862158
553.274729	-8.038921	72.867162
552.808893	-12.272682	72.872167
551.901153	-11.550782	72.877172
551.400644	-12.563700	72.882177
550.563412	-20.016689	72.887182
549.888029	-10.058001	72.892186
549.539186	-16.451840	72.897191
549.007154	-2.980554	72.902196
548.038284	-11.934294	72.907201
547.482083	-12.386421	72.912206
546.461084	-5.222147	72.917210
546.191207	-20.279489	72.922215
545.261820	-12.582624	72.927220
544.551703	-9.138920	72.932225
544.020563	-14.250075	72.937230
543.164617	0.556419	72.942234
543.459136	-5.348572	72.947239
542.395420	-8.622940	72.952244
541.551172	5.735431	72.957249
540.911367	-9.786523	72.962254
539.739182	-7.729425	72.967258
539.151410	-7.143646	72.972263
538.632467	-12.209437	72.977268
538.037085	-6.249915	72.982273
537.970345	-4.815185	72.987278
537.015029	-10.759181	72.992282
536.596120	-13.268967	72.997287
535.754928	-3.485703	73.002292
534.847605	-9.383729	73.007297
534.489769	-5.789567	73.012302
533.364592	-10.761933	73.017306
532.587126	-6.273043	73.022311
531.711343	-6.913946	73.027316
531.390208	-15.765866	73.032321
531.263201	-11.776405	73.037326
530.312776	-1.635124	73.042330
529.565452	-18.131812	73.047335
528.865590	-16.537876	73.052340
528.172695	-8.236878	73.057345
527.548404	-17.579804	73.062350
526.629123	4.586759	73.067354
526.356650	-5.242719	73.072359
525.713979	-7.682165	73.077364
525.095087	-1.764624	73.082369
524.169652	-8.463985	73.087374
523.230829	-4.729956	73.092378
523.008580	-12.982635	73.097383
522.389055	-7.320454	73.102388
521.464874	-10.960808	73.107393
521.164369	-15.282400	73.112398
520.359954	-15.464749	73.117402
520.007498	-11.333718	73.122407
518.832288	-5.647661	73.127412
517.874338	-12.322914	73.132417
517.652554	-21.266348	73.137422
517.107372	-4.938763	73.142426
516.655027	-12.164485	73.147431
515.622599	-10.747790	73.152436
514.864585	-15.852754	73.157441
514.680938	-11.075276	73.162446
513.363416	-6.642264	73.167450
512.641019	-17.619002	73.172455
512.199477	-4.209438	73.177460
511.810223	-12.088589	73.182465
511.703551	-4.366668	73.187470
510.706326	-10.624089	73.192474
509.879867	-20.452024	73.197479
508.889651	-11.422432	73.202484
507.999590	-11.149597	73.207489
507.738529	-8.628957	73.212494
506.919480	-16.097441	73.217498
506.749694	-16.281549	73.222503
505.835070	-20.678755	73.227508
504.975280	-16.936815	73.232513
504.789077	-14.429678	73.237518
503.717746	-15.559795	73.242522
503.226059	-13.641060	73.247527
502.277414	-14.524225	73.252532
501.844946	-12.346850	73.257537
501.633959	-12.956465	73.262542
500.689690	-13.058181	73.267546
499.851109	-25.377269	73.272551
499.437989	-16.759733	73.277556
498.144108	-17.106936	73.282561
497.550138	-20.410391	73.287566
496.604136	-7.981717	73.292570
496.407721	-14.634790	73.297575
495.974096	-9.443757	73.302580
495.697608	-3.232268	73.307585
495.146474	-17.191412	73.312590
494.381945	-12.247272	73.317594
493.307550	-20.933438	73.322599
492.465280	-16.500446	73.327604
492.083411	-19.457658	73.332609
491.117893	-21.768385	73.337614
490.075567	-5.057249	73.342618
489.728816	-11.915021	73.347623
489.275200	-18.304769	73.352628
488.738626	-8.685145	73.357633
487.966436	-24.121315	73.362638
486.879309	-9.740021	73.367642
486.597463	-17.565315	73.372647
486.071258	-8.850911	73.377652
485.499405	-8.611422	73.382657
485.079787	-14.730628	73.387662
483.972331	-16.342245	73.392666
483.268102	-22.559599	73.397671
482.328758	-10.207676	73.402676
481.597939	-11.863532	73.407681
481.420141	-18.344531	73.412686
480.939646	-11.077126	73.417690
480.276644	-8.259061	73.422695
479.494266	-10.647848	73.427700
478.580709	-13.911418	73.432705
478.429890	-14.436004	73.437710
476.963024	-7.465588	73.442714
476.538882	-16.548659	73.447719
475.886042	-14.306206	73.452724
475.595194	-12.152968	73.457729
474.749108	-15.324787	73.462734
473.875487	-12.504701	73.467738
473.626442	-15.765339	73.472743
473.420480	-9.133015	73.477748
472.057106	-6.083510	73.482753
471.610693	-12.204753	73.487758
470.813375	-15.292880	73.492762
470.062414	-14.674776	73.497767
469.039057	-17.832540	73.502772
468.770555	-16.244241	73.507777
468.556048	-15.136041	73.512782
467.249958	-13.781376	73.517786
466.513226	-16.210546	73.522791
465.800505	-8.187067	73.527796
465.592094	-15.077914	73.532801
465.262663	-16.042381	73.537806
463.992058	-14.187182	73.542810
463.832376	-14.811276	73.547815
463.229009	-14.733913	73.552820
461.820818	-12.624984	73.557825
460.901018	-14.872024	73.562830
460.305100	-12.506177	73.567834
460.352026	-23.051976	73.572839
459.892777	-20.753637	73.577844
459.191849	-12.065006	73.582849
458.449035	-10.137786	73.587854
457.816730	-14.233039	73.592858
456.873773	-14.618790	73.597863
455.798059	-7.291231	73.602868
455.110784	-21.720659	73.607873
454.643095	-10.303296	73.612878
454.267556	-14.061003	73.617882
453.787663	-13.719468	73.622887
453.275159	-20.640702	73.627892
452.624071	-7.328633	73.632897
452.109909	-24.051658	73.637902
451.094014	-14.894960	73.642906
450.258501	-21.529764	73.647911
449.733947	-16.333701	73.652916
448.475516	-22.842770	73.657921
448.153645	-19.180219	73.662926
447.220804	-13.844982	73.667930
447.185463	-24.186865	73.672935
446.533869	-21.151421	73.677940
445.273783	-16.481533	73.682945
444.627117	-18.434629	73.687950
444.271895	-20.899352	73.692954
443.993951	-24.642644	73.697959
443.412657	-13.519409	73.702964
442.347340	-5.766159	73.707969
441.857599	-20.006292	73.712974
441.302476	-15.259505	73.717978
440.580996	-13.474448	73.722983
439.650741	-16.905647	73.727988
439.055238	-7.633007	73.732993
438.207427	-15.230917	73.737998
437.004455	-13.206714	73.743002
436.894396	-24.905444	73.748007
436.663745	-18.970913	73.753012
436.119293	-14.344093	73.758017
435.317236	-23.480465	73.763022
434.499704	-14.090450	73.768026
433.933793	-18.822306	73.773031
433.412331	-19.445518	73.778036
432.322274	-12.274936	73.783041
431.991295	-18.160678	73.788046
431.112938	-7.740707	73.793050
430.600889	-13.987093	73.798055
429.491580	-15.800234	73.803060
428.842910	-24.454857	73.808065
428.861087	-14.862131	73.813070
427.262695	-12.275033	73.818074
426.952093	-20.683917	73.823079
426.371681	-21.873305	73.828084
425.880227	-18.644184	73.833089
425.562848	-21.706274	73.838094
424.628695	-17.838922	73.843098
423.657069	-17.545176	73.848103
423.304414	-9.033457	73.853108
423.064745	-18.964321	73.858113
422.160989	-22.940613	73.863118
421.155951	-8.949262	73.868122
420.744863	-12.899988	73.873127
419.876079	-14.409263	73.878132
418.543843	-12.132647	73.883137
418.458604	-20.765094	73.888142
418.116167	-12.933074	73.893146
417.551421	-15.627749	73.898151
416.358211	-14.562274	73.903156
415.850597	-11.428343	73.908161
415.526635	-14.333270	73.913166
414.816949	-20.352618	73.918170
414.095725	-23.665732	73.923175
413.382481	-19.355777	73.928180
412.715446	-19.771289	73.933185
411.918742	-12.168067	73.938190
411.344816	-7.072934	73.943194
410.660942	-16.447323	73.948199
410.372391	-16.328654	73.953204
409.200368	-18.937590	73.958209
408.604684	-16.576501	73.963214
407.882914	-7.925536	73.968218
407.705528	-18.572778	73.973223
406.772694	-12.819649	73.978228
405.798749	-12.509757	73.983233
406.054883	-19.827849	73.988238
404.568313	-21.211861	73.993242
403.834713	-22.931901	73.998247
403.350077	-12.664554	74.003252
402.721306	-15.557173	74.008257
402.233283	-24.784574	74.013262
400.952159	-12.237822	74.018266
400.536006	-19.503969	74.023271
400.182729	-19.810211	74.028276
399.419044	-10.394075	74.033281
399.225741	-20.308669	74.038286
397.898578	-20.478632	74.043290
397.175520	-9.788523	74.048295
397.032710	-22.306750	74.053300
396.471064	-18.478253	74.058305
395.659859	-28.166641	74.063310
395.182989	-16.074478	74.068314
394.230546	-21.120026	74.073319
393.189796	-21.668358	74.078324
392.590740	-21.479704	74.083329
392.285640	-27.014755	74.088334
391.332310	-18.369467	74.093338
390.657432	-27.669584	74.098343
390.440780	-24.353369	74.103348
389.352466	-18.061388	74.108353
389.241764	-23.796149	74.113358
388.119996	-16.060697	74.118362
387.651552	-22.851742	74.123367
387.246482	-24.679325	74.128372
385.809488	-18.350698	74.133377
385.118914	-27.224123	74.138382
384.570370	-16.079295	74.143386
384.532966	-17.107636	74.148391
383.995896	-19.649020	74.153396
382.837497	-10.529511	74.158401
382.243126	-27.220798	74.163406
381.565973	-29.309361	74.168410
380.820514	-17.792540	74.173415
379.896403	-22.508293	74.178420
379.161468	-19.536819	74.183425
379.163578	-18.860515	74.188430
378.524868	-11.444886	74.193434
378.284005	-16.977560	74.198439
377.042733	-22.596793	74.203444
376.292086	-9.339812	74.208449
376.208826	-20.926114	74.213454
374.733197	-13.753985	74.218458
374.507111	-14.574064	74.223463
374.346412	-19.651172	74.228468
372.809977	-15.131168	74.233473
372.316176	-16.667072	74.238478
371.987966	-10.510413	74.243482
370.997818	-6.197314	74.248487
370.400101	-16.504755	74.253492
369.432639	-8.372851	74.258497
369.309280	-18.300165	74.263502
367.883237	-6.107180	74.268506
367.316246	-11.231497	74.273511
366.926473	-16.440824	74.278516
366.321840	-13.778687	74.283521
366.221841	-18.461780	74.288526
364.811076	-7.204757	74.293530
364.373450	-21.163015	74.298535
364.142596	-11.038609	74.303540
363.130405	-17.563222	74.308545
362.181470	-23.880300	74.313550
361.340605	-15.396425	74.318554
361.057307	-5.836074	74.323559
360.969290	-15.124067	74.328564
360.003286	-10.329125	74.333569
359.384791	-22.322113	74.338574
358.577879	-16.007162	74.343578
357.961115	-19.532443	74.348583
356.935444	-19.103905	74.353588
356.151429	-12.984984	74.358593
355.827221	-10.370691	74.363598
355.503836	-20.081624	74.368602
354.481076	-22.804204	74.373607
354.022691	-15.106662	74.378612
353.486247	-19.639771	74.383617
352.489632	-25.017294	74.388622
351.526249	-17.945720	74.393626
351.178803	-24.426465	74.398631
350.969672	-26.252155	74.403636
349.613217	-1.008745	74.408641
349.301366	-28.173127	74.413646
348.557998	-18.321845	74.418650
348.217424	-14.273114	74.423655
347.567634	-18.162125	74.428660
346.303670	-13.584610	74.433665
345.753855	-17.510054	74.438670
345.295709	-18.745716	74.443674
344.860332	-17.545535	74.448679
343.885605	-22.748353	74.453684
342.929033	-8.666938	74.458689
343.028157	-25.717894	74.463694
342.108661	-14.867163	74.468698
341.054388	-25.082897	74.473703
340.974789	-27.407033	74.478708
340.264804	-18.824170	74.483713
339.226644	-25.117555	74.488718
338.398961	-20.384078	74.493722
338.080596	-27.787213	74.498727
337.628364	-17.017265	74.503732
336.427954	-23.650630	74.508737
335.769214	-20.044759	74.513742
335.020647	-10.820249	74.518746
334.965768	-19.817058	74.523751
334.140921	-9.492324	74.528756
332.870339	-15.622512	74.533761
332.742159	-20.651182	74.538766
331.938714	-7.035703	74.543770
331.688068	-22.234816	74.548775
330.789736	-21.173725	74.553780
330.007275	-11.021322	74.558785
329.747231	-21.822523	74.563790
328.926670	-19.174846	74.568794
327.975527	-16.848543	74.573799
327.609196	-21.702062	74.578804
327.013559	-10.242221	74.583809
326.029231	-20.393407	74.588814
325.121776	-12.837166	74.593818
324.605392	-21.736759	74.598823
324.640512	-16.916881	74.603828
323.364811	-10.229162	74.608833
322.627469	-16.674566	74.613838
322.015448	-9.898673	74.618842
321.809197	-14.787170	74.623847
321.079818	-19.746820	74.628852
319.905126	-9.729008	74.633857
319.760788	-19.798044	74.638862
318.955980	-18.769202	74.643866
317.803981	-12.334581	74.648871
317.618989	-19.883550	74.653876
316.508191	-15.548048	74.658881
316.317645	-14.678615	74.663886
315.752433	-8.624519	74.668890
314.954477	-16.708124	74.673895
314.111618	-12.137794	74.678900
313.528614	-2.496553	74.683905
312.819889	-12.833590	74.688910
312.117554	-20.538207	74.693914
310.813476	-2.672009	74.698919
310.974910	-12.009220	74.703924
310.526322	-10.313356	74.708929
310.528279	-6.946826	74.713934
309.209004	-9.108054	74.718938
308.448737	-4.084121	74.723943
307.502115	-8.386264	74.728948
306.717988	-10.271680	74.733953
306.456887	-5.861885	74.738958
305.786568	-9.102658	74.743962
304.667401	-20.241559	74.748967
304.299828	-23.114284	74.753972
303.540647	-16.001129	74.758977
303.392074	-18.394693	74.763982
301.977055	-14.450648	74.768986
301.283916	-24.924193	74.773991
301.063307	-15.392763	74.778996
300.514296	-17.787149	74.784001
299.971839	-21.494563	74.789006
298.918354	-7.779300	74.794010
298.516547	-4.293218	74.799015
298.018205	-15.756577	74.804020
296.781158	-18.020787	74.809025
296.396839	-18.869251	74.814030
295.569766	-25.732408	74.819034
295.086147	-11.491417	74.824039
294.640646	-15.622705	74.829044
293.279777	-12.362202	74.834049
293.185777	-21.124119	74.839054
292.570484	-9.186492	74.844058
291.743831	-14.187395	74.849063
291.444748	-16.176932	74.854068
290.369678	-17.648546	74.859073
290.221950	-13.914393	74.864078
289.099959	-18.114455	74.869082
288.420335	-13.275258	74.874087
288.223015	-24.231521	74.879092
286.844657	-12.829827	74.884097
286.363714	-21.055413	74.889102
285.810824	-17.480596	74.894106
285.016689	-16.311522	74.899111
284.903727	-17.255278	74.904116
283.492188	-8.440720	74.909121
282.880299	-23.741500	74.914126
282.527486	-11.968714	74.919130
282.321560	-14.794667	74.924135
281.492336	-15.802434	74.929140
280.530725	-21.710613	74.934145
280.183706	-22.399445	74.939150
279.006774	-13.363674	74.944154
278.068363	-17.481036	74.949159
277.497971	-15.636443	74.954164
277.275752	-13.451551	74.959169
277.086427	-14.346864	74.964174
275.736484	-0.297333	74.969178
275.341924	-16.296639	74.974183
274.861069	-6.133955	74.979188
273.953630	-1.764621	74.984193
273.490806	-2.917525	74.989198
272.194816	-11.500447	74.994202
271.984847	-5.714278	74.999207
271.538871	-13.928092	75.004212
270.534264	-8.718547	75.009217
270.144979	-15.460683	75.014222
269.639167	-6.829926	75.019226
268.512121	-3.103650	75.024231
267.914173	-22.195951	75.029236
266.918613	-10.965654	75.034241
266.819993	-9.007037	75.039246
266.327953	-12.610522	75.044250
265.410053	-11.987821	75.049255
265.195369	-11.344763	75.054260
263.775048	-17.205042	75.059265
262.831607	-19.689499	75.064270
262.027475	-19.159047	75.069274
261.815703	-21.690760	75.074279
261.477952	-24.043122	75.079284
261.086621	-12.882343	75.084289
260.485921	-28.981227	75.089294
259.725301	-19.308522	75.094298
259.052420	-15.845453	75.099303
257.999725	-21.292839	75.104308
257.062049	-18.915042	75.109313
256.879104	-33.123582	75.114318
256.331858	-8.387619	75.119322
255.312612	-11.579058	75.124327
254.557669	-17.845017	75.129332
253.808789	-14.836594	75.134337
253.655334	-17.126876	75.139342
253.211352	-24.576199	75.144346
251.917392	-19.938668	75.149351
251.447122	-20.763960	75.154356
251.075355	-13.365636	75.159361
250.349528	-23.111728	75.164366
249.511805	-24.471354	75.169370
248.714911	-17.561903	75.174375
248.493133	-24.583039	75.179380
247.007317	-19.508079	75.184385
246.805511	-26.030943	75.189390
246.014111	-12.658641	75.194394
245.606614	-22.452327	75.199399
245.196607	-24.749014	75.204404
244.271319	-21.321394	75.209409
243.904231	-33.283448	75.214414
243.260332	-18.253689	75.219418
241.935001	-13.910762	75.224423
241.343460	-22.840923	75.229428
240.752718	-16.986169	75.234433
240.455042	-18.471313	75.239438
239.597436	-14.210838	75.244442
238.695620	-21.684935	75.249447
238.473085	-22.612796	75.254452
237.729002	-14.432892	75.259457
237.185508	-19.866834	75.264462
236.311843	-20.765001	75.269466
235.685601	-18.902035	75.274471
235.012359	-19.627157	75.279476
234.144307	-20.398490	75.284481
233.540551	-10.766551	75.289486
233.363270	-11.364170	75.294490
232.447394	-17.151891	75.299495
231.527011	-13.639895	75.304500
230.358741	-10.924136	75.309505
230.344444	-25.982708	75.314510
229.826694	-15.025694	75.319514
228.715824	-7.004919	75.324519
228.125125	-14.659500	75.329524
227.738115	-7.436930	75.334529
227.323040	-25.340994	75.339534
226.594524	-8.673523	75.344538
225.638696	-9.205361	75.349543
225.394564	-19.195395	75.354548
224.584686	-7.154198	75.359553
223.411450	-18.960924	75.364558
222.709260	-7.709578	75.369562
222.164996	-5.731948	75.374567
222.206981	-11.357002	75.379572
221.229349	-7.093151	75.384577
220.364697	-12.877998	75.389582
219.676181	-13.711064	75.394586
219.252729	-9.043576	75.399591
218.942790	-16.473265	75.404596
217.385120	-17.637674	75.409601
217.320915	-16.111885	75.414606
216.584285	-25.193940	75.419610
215.593508	-28.008286	75.424615
215.147573	-18.773661	75.429620
214.534328	-19.232386	75.434625
214.097880	-18.216510	75.439630
213.010402	-19.610418	75.444634
212.102623	-16.543535	75.449639
212.106428	-24.587772	75.454644
211.495224	-8.440459	75.459649
210.768963	-27.034466	75.464654
209.741744	-24.990873	75.469658
208.994149	-17.395435	75.474663
208.852422	-26.307418	75.479668
207.593761	-9.314154	75.484673
207.065296	-25.031888	75.489678
206.690445	-16.461432	75.494682
206.149830	-13.763737	75.499687
205.299188	-22.177927	75.504692
204.237467	-25.594372	75.509697
203.979220	-19.056212	75.514702
203.866235	-23.546413	75.519706
202.851453	-13.210292	75.524711
202.147514	-28.658776	75.529716
200.854347	-18.316118	75.534721
200.174191	-15.673441	75.539726
199.452908	-23.267765	75.544730
198.956099	-21.721885	75.549735
198.830695	-19.686461	75.554740
198.218777	-15.892487	75.559745
197.855928	-23.010967	75.564750
196.785276	-20.183030	75.569754
196.073435	-15.001218	75.574759
195.680902	-22.633765	75.579764
194.646930	-13.869908	75.584769
194.139240	-24.092290	75.589774
193.531347	-11.607071	75.594778
192.186183	-14.579363	75.599783
191.804611	-30.194355	75.604788
191.218092	-15.646807	75.609793
190.810350	-26.036506	75.614798
190.618423	-14.193182	75.619802
189.635840	-20.517432	75.624807
189.004515	-16.766093	75.629812
188.060222	-15.916812	75.634817
186.983172	-32.786505	75.639822
186.229397	-10.714119	75.644826
186.254279	-16.263904	75.649831
185.713109	-16.286273	75.654836
184.843170	-13.706369	75.659841
184.208049	-26.300589	75.664846
183.481923	-14.127669	75.669850
182.877489	-20.335598	75.674855
181.951989	-20.843870	75.679860
180.932809	-13.425886	75.684865
180.850641	-31.379853	75.689870
180.453793	-20.109390	75.694874
179.634017	-22.165690	75.699879
178.844379	-32.991211	75.704884
178.215444	-19.256890	75.709889
178.056383	-23.985738	75.714894
176.812776	-19.521775	75.719898
176.295724	-22.831097	75.724903
175.482634	-23.913937	75.729908
174.613495	-22.442720	75.734913
173.983440	-31.571709	75.739918
173.402436	-21.572825	75.744922
172.676823	-22.382616	75.749927
172.728939	-28.625845	75.754932
171.128775	-18.674178	75.759937
170.666902	-26.868075	75.764942
170.460407	-23.644929	75.769946
169.802414	-24.839228	75.774951
168.900772	-19.554609	75.779956
168.135109	-22.346485	75.784961
167.801191	-20.306196	75.789966
166.950987	-25.317483	75.794970
166.052953	-21.782223	75.799975
165.492799	-40.863132	75.804980
164.815578	-26.408359	75.809985
164.541520	-19.158072	75.814990
164.151137	-29.903754	75.819994
163.240069	-22.572391	75.824999
162.403287	-25.747150	75.830004
161.351594	-14.326531	75.835009
161.124747	-29.420578	75.840014
160.713886	-28.793538	75.845018
159.650629	-25.648232	75.850023
159.142391	-32.374520	75.855028
157.985201	-15.969843	75.860033
157.698667	-24.216928	75.865038
157.458530	-24.082297	75.870042
156.500498	-25.430590	75.875047
155.803064	-24.538662	75.880052
155.159954	-27.271231	75.885057
154.454215	-26.078367	75.890062
153.763775	-17.326702	75.895066
153.048534	-17.706070	75.900071
152.706176	-22.489262	75.905076
150.846339	-15.788743	75.910081
150.542825	-26.557737	75.915086
150.046164	-26.185086	75.920090
149.564030	-14.629791	75.925095
149.420871	-23.729189	75.930100
148.961687	-10.064502	75.935105
148.265456	-20.769299	75.940110
147.449295	-15.704878	75.945114
146.391562	-15.849862	75.950119
145.528048	-29.986121	75.955124
144.694986	-17.728338	75.960129
144.437692	-22.293289	75.965134
144.181004	-21.629332	75.970138
143.173713	-14.574342	75.975143
142.395122	-24.594240	75.980148
141.460255	-12.935209	75.985153
141.413358	-16.680609	75.990158
141.067507	-19.812226	75.995162
139.860741	-14.097329	76.000167
139.306431	-16.047721	76.005172
138.857638	-18.074860	76.010177
137.934254	-25.006170	76.015182
137.361084	-22.951378	76.020186
136.520025	-23.082026	76.025191
135.579896	-18.138178	76.030196
134.605403	-20.116175	76.035201
134.303213	-26.687665	76.040206
133.921411	-25.713606	76.045210
133.584156	-13.567998	76.050215
133.255810	-27.212450	76.055220
131.818394	-14.842517	76.060225
131.569799	-28.862372	76.065230
130.335166	-22.581654	76.070234
129.351825	-24.615006	76.075239
128.976608	-16.389828	76.080244
128.359792	-12.057335	76.085249
128.340579	-18.409035	76.090254
127.859655	-24.546759	76.095258
126.478916	-13.157230	76.100263
126.033363	-29.859521	76.105268
125.133567	-18.314890	76.110273
124.481181	-27.659491	76.115278
124.042635	-23.011665	76.120282
123.149932	-23.422645	76.125287
123.237308	-29.039158	76.130292
122.110311	-22.266262	76.135297
121.302429	-18.439445	76.140302
120.918619	-32.800417	76.145306
120.145281	-17.395201	76.150311
119.210042	-23.370587	76.155316
118.733057	-15.759939	76.160321
118.330668	-21.624767	76.165326
117.698122	-19.191506	76.170330
116.536450	-17.569541	76.175335
116.146853	-24.371510	76.180340
115.386618	-25.089032	76.185345
114.406071	-10.292560	76.190350
113.731462	-16.609123	76.195354
112.869240	-12.710560	76.200359
112.627768	-17.801561	76.205364
112.246070	-14.432202	76.210369
112.062310	-20.939002	76.215374
110.957106	-16.317313	76.220378
110.349957	-17.902891	76.225383
109.831525	-19.952033	76.230388
108.655096	-19.213929	76.235393
108.070642	-17.073755	76.240398
107.558963	-20.738720	76.245402
106.734999	-13.301383	76.250407
106.185300	-23.253695	76.255412
105.118345	-17.524814	76.260417
104.702148	-23.294398	76.265422
104.595598	-32.484774	76.270426
103.367039	-17.820636	76.275431
102.724298	-26.867156	76.280436
102.201509	-17.353769	76.285441
101.722334	-24.765900	76.290446
101.203879	-27.956711	76.295450
100.342538	-19.124166	76.300455
99.922260	-24.831599	76.305460
98.695967	-23.364895	76.310465
97.935440	-22.259469	76.315470
97.404134	-18.243373	76.320474
96.977272	-15.190074	76.325479
96.767467	-21.522412	76.330484
95.466349	-18.458988	76.335489
94.725691	-13.023406	76.340494
94.379195	-12.531195	76.345498
93.855449	-11.348416	76.350503
92.735481	-19.759027	76.355508
92.196972	-14.628488	76.360513
91.760012	-14.678495	76.365518
91.194988	-19.746274	76.370522
89.995097	-12.696817	76.375527
89.498773	-23.547008	76.380532
88.944409	-11.574923	76.385537
88.709230	-21.219436	76.390542
87.736858	-18.511205	76.395546
86.839283	-17.308226	76.400551
86.658557	-20.984969	76.405556
85.610174	-19.809976	76.410561
84.913075	-23.770203	76.415566
84.304078	-28.515584	76.420570
83.567634	-15.853742	76.425575
83.482885	-24.874137	76.430580
82.472841	-17.861266	76.435585
81.584397	-20.609877	76.440590
81.255764	-12.729581	76.445594
80.262492	-15.128747	76.450599
79.539965	-19.833945	76.455604
78.914135	-18.694805	76.460609
78.632685	-14.718555	76.465614
78.072413	-13.384872	76.470618
77.042810	-22.131573	76.475623
76.730055	-22.319654	76.480628
76.155760	-7.099126	76.485633
75.303290	-15.145553	76.490638
74.569024	-14.307650	76.495642
73.979112	-20.867933	76.500647
73.015721	-21.773806	76.505652
71.641523	-20.652493	76.510657
71.139524	-14.196871	76.515662
70.954665	-18.948400	76.520666
70.458910	-9.664813	76.525671
70.460961	-15.046953	76.530676
69.535350	-19.100036	76.535681
68.719553	-23.676817	76.540686
68.109532	-23.070034	76.545690
67.289910	-16.924862	76.550695
66.904076	-18.145194	76.555700
65.984001	-13.349594	76.560705
64.839005	-22.787489	76.565710
64.037368	-18.061241	76.570714
63.310685	-17.562001	76.575719
63.510925	-13.656271	76.580724
62.865940	-15.317799	76.585729
62.167042	-13.909965	76.590734
61.315090	-14.004159	76.595738
60.556408	-17.820521	76.600743
60.300243	-18.929074	76.605748
59.355637	-16.203183	76.610753
58.805278	-21.166063	76.615758
58.239127	-25.538238	76.620762
57.025688	-17.160436	76.625767
56.270528	-32.417759	76.630772
55.458275	-18.898605	76.635777
55.745208	-27.208753	76.640782
55.072004	-20.451443	76.645786
53.824222	-20.186041	76.650791
53.782037	-23.648342	76.655796
52.672167	-17.355950	76.660801
51.476613	-22.487143	76.665806
50.925089	-21.948031	76.670810
50.395706	-27.929775	76.675815
50.195153	-32.196263	76.680820
49.495033	-16.551987	76.685825
48.819430	-22.079916	76.690830
48.347980	-23.699735	76.695834
47.880588	-27.781741	76.700839
47.041209	-25.902081	76.705844
45.830375	-26.227597	76.710849
45.343688	-23.171057	76.715854
44.975457	-27.626835	76.720858
44.182364	-25.836555	76.725863
43.291526	-22.106867	76.730868
42.670772	-22.255277	76.735873
42.366429	-32.606230	76.740878
41.288303	-27.591458	76.745882
40.317747	-27.100619	76.750887
39.991827	-29.317641	76.755892
39.227514	-25.642826	76.760897
38.884442	-32.573614	76.765902
37.776966	-32.172894	76.770906
37.359423	-24.521262	76.775911
37.414035	-32.163590	76.780916
36.717474	-24.265609	76.785921
35.803436	-19.698038	76.790926
35.359985	-28.050948	76.795930
33.926888	-26.749915	76.800935
33.389326	-28.830678	76.805940
32.936163	-26.140594	76.810945
32.048091	-17.888796	76.815950
31.403196	-31.733449	76.820954
30.553336	-24.867535	76.825959
30.425323	-32.146429	76.830964
30.100791	-27.830582	76.835969
28.757669	-26.442976	76.840974
28.119964	-33.962254	76.845978
27.418241	-36.590819	76.850983
27.376950	-37.709989	76.855988
26.196683	-22.667193	76.860993
25.257684	-34.205230	76.865998
24.955419	-34.134790	76.871002
24.293801	-25.042361	76.876007
23.572802	-29.135945	76.881012
22.722728	-24.326270	76.886017
22.006885	-30.077995	76.891022
21.967139	-27.393934	76.896026
20.883295	-33.110609	76.901031
20.463920	-39.794260	76.906036
19.683159	-33.131752	76.911041
18.783442	-27.976702	76.916046
18.622026	-21.468175	76.921050
17.545100	-21.658926	76.926055
16.975389	-32.645608	76.931060
16.391421	-22.024934	76.936065
15.806080	-31.425918	76.941070
15.169884	-21.487593	76.946074
14.271382	-20.582475	76.951079
13.841196	-34.186987	76.956084
12.758899	-21.268125	76.961089
11.878109	-29.983334	76.966094
11.589694	-28.745043	76.971098
10.974046	-27.804622	76.976103
10.679545	-28.394562	76.981108
10.137104	-18.026505	76.986113
9.215439	-28.636933	76.991118
8.686607	-26.600226	76.996122
7.339124	-31.778115	77.001127
6.709017	-31.002539	77.006132
6.254669	-20.238543	77.011137
5.796021	-31.198786	77.016142
5.578218	-20.275412	77.021147
4.322609	-28.309528	77.026151
3.882577	-23.260917	77.031156
3.310119	-38.588352	77.036161