Mon Mar 08 18:14:55 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.085979	96.575788	0.000000
-0.208654	87.070988	0.005005
-0.750258	66.396036	0.010010
-2.399932	25.128579	0.015014
-6.405993	11.616674	0.020019
-12.014419	18.267075	0.025024
-17.434272	14.593453	0.030029
-21.513222	13.996917	0.035034
-25.313759	14.095538	0.040038
-29.580992	19.234248	0.045043
-32.981958	7.237453	0.050048
-36.574927	16.210842	0.055053
-40.021499	18.350286	0.060058
-43.554587	15.451173	0.065062
-47.495644	31.798475	0.070067
-51.269763	22.474137	0.075072
-55.468967	17.880498	0.080077
-58.941847	21.356639	0.085082
-62.355306	18.403777	0.090086
-66.229477	22.634629	0.095091
-70.044932	16.625242	0.100096
-73.839397	18.254132	0.105101
-77.948523	15.730814	0.110106
-81.796529	19.063417	0.115110
-85.281383	20.881038	0.120115
-88.477354	10.956770	0.125120
-92.732706	6.127741	0.130125
-96.611518	12.622216	0.135130
-100.440403	7.450779	0.140134
-104.456003	11.731059	0.145139
-107.933854	14.898991	0.150144
-111.258767	11.011169	0.155149
-115.009667	15.930450	0.160154
-119.033459	8.765413	0.165158
-122.686340	16.408124	0.170163
-126.786708	-0.731121	0.175168
-130.899836	1.659880	0.180173
-134.923733	15.027573	0.185178
-138.222425	16.616876	0.190182
-141.828166	18.662017	0.195187
-145.244409	7.273359	0.200192
-149.350968	16.540161	0.205197
-153.195736	10.802086	0.210202
-156.908887	15.548255	0.215206
-160.739624	10.965391	0.220211
-164.242489	13.839361	0.225216
-167.842327	17.845249	0.230221
-171.848306	10.697961	0.235226
-175.548832	13.062617	0.240230
-179.924630	23.365879	0.245235
-183.162582	4.550060	0.250240
-186.623846	17.656164	0.255245
-190.549630	23.533834	0.260250
-194.200068	12.122701	0.265254
-198.289282	24.425483	0.270259
-201.870572	10.338384	0.275264
-205.886691	21.374307	0.280269
-209.331658	10.703083	0.285274
-212.896128	18.182009	0.290278
-216.796352	18.408800	0.295283
-220.569503	8.937949	0.300288
-224.492385	8.296349	0.305293
-228.774836	16.952712	0.310298
-231.843422	3.244290	0.315302
-235.660965	11.444852	0.320307
-239.461390	7.360308	0.325312
-243.494777	9.549545	0.330317
-246.890826	2.268772	0.335322
-250.580877	1.810817	0.340326
-255.189036	17.493785	0.345331
-258.735932	18.637187	0.350336
-261.984739	10.684829	0.355341
-265.999158	20.736595	0.360346
-269.294141	14.400042	0.365350
-273.100662	11.246888	0.370355
-277.249340	14.481139	0.375360
-281.085125	21.713323	0.380365
-284.789959	21.850689	0.385370
-288.155272	12.527726	0.390374
-292.251893	23.385832	0.395379
-296.039400	15.726085	0.400384
-299.780973	21.946666	0.405389
-303.825831	16.188743	0.410394
-307.074414	21.867030	0.415398
-310.981339	18.171746	0.420403
-314.656497	17.520707	0.425408
-318.586454	12.321610	0.430413
-322.561740	14.738236	0.435418
-325.832544	15.601126	0.440422
-330.058533	17.277230	0.445427
-333.732293	9.206746	0.450432
-337.303638	7.793302	0.455437
-341.210213	17.203519	0.460442
-345.072612	17.419748	0.465446
-348.830707	25.107969	0.470451
-352.246749	16.803984	0.475456
-356.026702	17.514825	0.480461
-360.014950	24.173832	0.485466
-363.395855	4.717249	0.490470
-367.574848	6.849517	0.495475
-371.312401	15.018591	0.500480
-375.051421	14.554454	0.505485
-379.066508	19.916843	0.510490
-382.698668	6.030549	0.515494
-386.507469	13.851491	0.520499
-389.624454	10.607350	0.525504
-393.548849	20.036263	0.530509
-397.427207	21.103489	0.535514
-401.285259	6.270895	0.540518
-405.287371	14.023388	0.545523
-408.890788	15.246995	0.550528
-412.922914	14.974794	0.555533
-416.426362	21.729934	0.560538
-419.807388	16.949532	0.565542
-423.907717	21.393668	0.570547
-427.233965	9.798693	0.575552
-431.603987	16.894075	0.580557
-435.568412	22.824030	0.585562
-439.165420	15.622937	0.590566
-442.820505	13.351007	0.595571
-446.601675	16.266670	0.600576
-450.233018	18.726346	0.605581
-454.256095	17.722672	0.610586
-457.546683	-1.432796	0.615590
-461.460546	12.307310	0.620595
-465.140798	17.316757	0.625600
-469.203920	16.519767	0.630605
-472.897014	22.972551	0.635610
-476.401894	18.469045	0.640614
-480.117140	19.647543	0.645619
-483.946017	12.097217	0.650624
-487.834617	18.136564	0.655629
-491.998407	14.372227	0.660634
-495.388613	9.396295	0.665638
-498.932465	17.167207	0.670643
-502.553519	12.398458	0.675648
-506.654344	10.588889	0.680653
-510.661719	19.056721	0.685658
-514.446564	8.553796	0.690662
-518.443993	15.774313	0.695667
-521.575263	12.125795	0.700672
-525.100872	6.805698	0.705677
-528.762942	12.717465	0.710682
-532.616593	9.444534	0.715686
-536.977163	16.216907	0.720691
-540.594258	7.081198	0.725696
-544.551495	13.338167	0.730701
-548.525105	18.908663	0.735706
-552.027503	8.892094	0.740710
-555.718133	17.673660	0.745715
-559.269600	21.169368	0.750720
-563.072818	23.571517	0.755725
-566.957313	13.582893	0.760730
-570.429642	11.346620	0.765734
-574.439421	21.590509	0.770739
-577.944822	15.981846	0.775744
-581.566787	24.542759	0.780749
-585.834492	17.825918	0.785754
-589.696974	15.874342	0.790758
-593.487374	11.228981	0.795763
-596.958754	12.315087	0.800768
-600.547065	13.482954	0.805773
-604.480393	11.992133	0.810778
-608.284875	2.460717	0.815782
-612.170439	19.403909	0.820787
-615.674950	6.686581	0.825792
-619.622292	10.026435	0.830797
-623.437251	15.835042	0.835802
-626.735433	5.029065	0.840806
-630.770949	12.954403	0.845811
-634.107422	1.799759	0.850816
-638.370057	16.951975	0.855821
-642.465753	10.313412	0.860826
-645.734092	11.244151	0.865830
-649.801003	11.447821	0.870835
-653.409191	14.441817	0.875840
-656.935349	24.029848	0.880845
-661.240832	11.186695	0.885850
-664.382876	-2.588204	0.890854
-668.652839	12.983101	0.895859
-672.082805	9.395132	0.900864
-675.911277	13.625944	0.905869
-679.585613	9.252326	0.910874
-683.086047	7.834384	0.915878
-687.175922	14.104892	0.920883
-690.898450	6.293510	0.925888
-694.701201	15.161000	0.930893
-699.063203	5.622639	0.935898
-702.523232	7.306298	0.940902
-706.243805	10.651055	0.945907
-709.717645	9.131135	0.950912
-713.687365	10.498889	0.955917
-717.330590	14.375326	0.960922
-720.610071	5.797787	0.965926
-725.030466	11.599230	0.970931
-728.671260	6.179591	0.975936
-732.202897	10.134406	0.980941
-736.029511	13.075128	0.985946
-739.871759	9.354463	0.990950
-743.435561	14.900776	0.995955
-747.136416	10.939916	1.000960
-751.523489	17.707442	1.005965
-755.413522	18.736116	1.010970
-758.483358	8.966118	1.015974
-762.663630	13.056184	1.020979
-766.360191	16.868683	1.025984
-769.791847	14.965236	1.030989
-773.877819	18.332231	1.035994
-777.519271	18.480733	1.040998
-781.534638	21.435930	1.046003
-784.501545	14.118907	1.051008
-788.228558	24.761042	1.056013
-792.508219	21.052033	1.061018
-796.119367	16.370469	1.066022
-800.367285	25.988917	1.071027
-803.797298	25.433488	1.076032
-807.779363	17.023567	1.081037
-811.599150	15.518099	1.086042
-815.165732	8.811040	1.091046
-819.121385	18.275568	1.096051
-822.484597	23.430405	1.101056
-826.134750	15.700710	1.106061
-830.550485	21.239842	1.111066
-833.870117	13.285444	1.116070
-837.606367	16.946709	1.121075
-841.454024	18.777688	1.126080
-845.041795	19.835456	1.131085
-848.996074	21.314504	1.136090
-852.877917	19.355420	1.141094
-857.006066	27.265981	1.146099
-860.246577	16.367555	1.151104
-864.090264	10.791343	1.156109
-867.809268	22.608663	1.161114
-871.484163	26.302748	1.166118
-875.237733	28.621766	1.171123
-878.959851	20.042684	1.176128
-882.988608	18.900310	1.181133
-886.990025	21.651612	1.186138
-890.171637	15.364068	1.191142
-894.213194	23.185154	1.196147
-897.866257	7.161672	1.201152
-901.743397	12.553318	1.206157
-905.690351	17.822100	1.211162
-908.886930	3.226842	1.216166
-913.119170	22.878211	1.221171
-916.832528	13.698583	1.226176
-920.394999	7.716399	1.231181
-923.863759	17.172622	1.236186
-927.514592	10.051880	1.241190
-931.849298	15.229748	1.246195
-935.343938	-1.452896	1.251200
-939.220099	10.298189	1.256205
-943.424290	21.906210	1.261210
-946.615640	6.941180	1.266214
-950.442135	8.570264	1.271219
-954.294516	6.936210	1.276224
-958.048821	4.359276	1.281229
-962.058152	8.092784	1.286234
-965.892009	2.087844	1.291238
-969.399994	14.377736	1.296243
-972.888730	8.618798	1.301248
-976.432748	7.553602	1.306253
-980.675640	16.316881	1.311258
-984.364882	1.655454	1.316262
-988.274189	3.772482	1.321267
-992.119384	11.287943	1.326272
-995.709693	14.169213	1.331277
-999.638023	13.966567	1.336282
-1002.939538	-4.921355	1.341286
-1007.014686	14.205159	1.346291
-1010.899374	11.765851	1.351296
-1014.529105	5.751998	1.356301
-1018.378043	16.502271	1.361306
-1021.819736	15.843380	1.366310
-1025.759723	13.833967	1.371315
-1029.279678	0.503233	1.376320
-1033.418408	11.285683	1.381325
-1037.490205	13.433513	1.386330
-1040.475989	15.857055	1.391334
-1044.342327	11.547850	1.396339
-1048.212773	7.556261	1.401344
-1052.074061	13.010264	1.406349
-1055.982632	12.340951	1.411354
-1059.340203	7.576674	1.416358
-1063.467153	15.410116	1.421363
-1067.181178	5.472379	1.426368
-1071.044008	8.061480	1.431373
-1075.074990	19.632551	1.436378
-1078.355902	7.867335	1.441382
-1082.058844	14.685282	1.446387
-1085.840404	10.504504	1.451392
-1089.439197	2.308165	1.456397
-1093.787343	9.543136	1.461402
-1097.422031	3.730476	1.466406
-1101.197615	7.027876	1.471411
-1104.796630	8.363790	1.476416
-1108.391551	2.434405	1.481421
-1112.086663	12.127358	1.486426
-1115.783124	14.290968	1.491430
-1119.847685	9.542119	1.496435
-1123.778249	10.111130	1.501440
-1127.136470	9.096861	1.506445
-1131.241920	6.003984	1.511450
-1135.027489	13.809736	1.516454
-1138.770444	8.339298	1.521459
-1142.528172	13.253355	1.526464
-1145.878385	13.040460	1.531469
-1149.891179	16.532001	1.536474
-1153.538040	8.521640	1.541478
-1157.737043	9.770714	1.546483
-1161.441442	16.278371	1.551488
-1164.997150	2.087879	1.556493
-1168.563083	16.927657	1.561498
-1171.933595	8.381126	1.566502
-1176.162726	11.200886	1.571507
-1179.980422	18.650748	1.576512
-1184.095547	17.041771	1.581517
-1187.659711	14.214025	1.586522
-1191.130691	-3.124795	1.591526
-1195.143157	2.079247	1.596531
-1198.920458	8.814655	1.601536
-1202.489989	17.196194	1.606541
-1206.708689	20.381752	1.611546
-1210.062583	11.337482	1.616550
-1213.746254	4.610379	1.621555
-1217.542404	10.352251	1.626560
-1221.535118	12.462514	1.631565
-1225.081705	7.739771	1.636570
-1228.393899	10.453890	1.641574
-1232.642331	19.888662	1.646579
-1236.222758	10.978450	1.651584
-1239.869005	9.529493	1.656589
-1244.244327	9.953852	1.661594
-1247.840050	1.624825	1.666598
-1251.847085	15.966058	1.671603
-1255.387119	13.571350	1.676608
-1258.775707	14.102735	1.681613
-1262.827651	17.991797	1.686618
-1266.250133	2.099211	1.691622
-1269.972795	11.997070	1.696627
-1274.306658	20.512079	1.701632
-1278.005653	13.152053	1.706637
-1281.563814	13.827300	1.711642
-1284.862410	16.458903	1.716646
-1288.643944	13.076357	1.721651
-1292.600875	11.844358	1.726656
-1296.825202	12.396028	1.731661
-1300.904154	8.042450	1.736666
-1304.054172	0.255580	1.741670
-1308.009230	12.734182	1.746675
-1311.475163	8.667259	1.751680
-1315.196248	9.725007	1.756685
-1319.364004	16.881053	1.761690
-1322.858578	12.943303	1.766694
-1326.981998	21.366378	1.771699
-1330.704913	10.107519	1.776704
-1334.249288	6.772240	1.781709
-1338.032823	9.926218	1.786714
-1341.300837	3.739887	1.791718
-1345.347346	8.347270	1.796723
-1349.049768	8.189474	1.801728
-1352.879846	15.726737	1.806733
-1356.944062	13.718859	1.811738
-1360.821255	0.680819	1.816742
-1364.221153	-0.357968	1.821747
-1367.882266	-0.292124	1.826752
-1371.927953	11.677567	1.831757
-1375.987245	14.093626	1.836762
-1379.337522	1.669818	1.841766
-1383.239159	6.088500	1.846771
-1386.904428	12.091946	1.851776
-1390.397513	14.871522	1.856781
-1394.112453	10.221728	1.861786
-1397.779020	16.252207	1.866790
-1401.961924	12.930957	1.871795
-1405.532759	7.856011	1.876800
-1409.156048	3.478561	1.881805
-1413.466839	11.140189	1.886810
-1417.287703	10.173611	1.891814
-1421.077231	21.408554	1.896819
-1424.709405	21.471431	1.901824
-1427.864984	5.049123	1.906829
-1431.703257	8.068522	1.911834
-1435.311706	4.228027	1.916838
-1439.727695	16.047399	1.921843
-1443.628355	9.741755	1.926848
-1446.941997	15.020399	1.931853
-1450.770267	18.352025	1.936858
-1454.229869	14.419919	1.941862
-1458.020824	11.329310	1.946867
-1461.984742	11.921581	1.951872
-1465.813038	14.789636	1.956877
-1470.016585	11.050796	1.961882
-1473.353221	8.549747	1.966886
-1477.173825	22.147167	1.971891
-1480.910378	16.592702	1.976896
-1484.413608	1.161241	1.981901
-1488.697629	11.092556	1.986906
-1492.268280	9.559361	1.991910
-1496.079327	14.421015	1.996915
-1499.826333	19.332721	2.006912
-1500.813431	12.878660	2.016909
-1498.440025	11.984089	2.026906
-1495.505335	13.739000	2.036902
-1493.112598	11.658753	2.046899
-1491.426139	15.287182	2.056896
-1489.623463	12.988812	2.066893
-1487.789941	18.677823	2.076890
-1485.742609	12.764101	2.086886
-1483.969145	18.394840	2.096883
-1482.012506	18.743295	2.106880
-1479.678666	17.585090	2.116877
-1478.351917	14.767701	2.126874
-1476.375239	12.840936	2.136870
-1474.303352	17.407093	2.146867
-1472.490661	11.253073	2.156864
-1470.715108	14.008337	2.166861
-1468.873426	18.701359	2.176858
-1466.949382	12.891076	2.186854
-1464.874006	14.842048	2.196851
-1462.859257	5.393704	2.206848
-1460.943431	14.607838	2.216845
-1459.245196	13.218285	2.226842
-1457.471891	14.808702	2.236838
-1455.532915	15.816825	2.246835
-1453.571558	8.486428	2.256832
-1451.580822	8.957338	2.266829
-1449.810377	13.833880	2.276826
-1447.735489	10.884084	2.286822
-1446.127648	8.152754	2.296819
-1444.508347	9.969937	2.306816
-1442.254460	10.679762	2.316813
-1440.535372	9.692658	2.326810
-1438.381372	13.543096	2.336806
-1436.659981	6.716906	2.346803
-1434.831830	10.801093	2.356800
-1432.743226	14.197815	2.366797
-1430.863400	10.587714	2.376794
-1429.203957	15.107850	2.386790
-1427.342815	4.631011	2.396787
-1425.384370	9.685883	2.406784
-1423.557441	8.580477	2.416781
-1421.740603	8.214027	2.426778
-1419.868089	7.426575	2.436774
-1417.798780	8.830688	2.446771
-1416.062708	13.022788	2.456768
-1413.711086	11.133934	2.466765
-1412.102236	8.760872	2.476762
-1410.559581	13.086571	2.486758
-1408.459451	3.291455	2.496755
-1406.555963	15.461711	2.506752
-1404.841384	13.548548	2.516749
-1402.791893	13.744842	2.526746
-1400.974445	10.485791	2.536742
-1399.115338	14.680311	2.546739
-1396.936809	10.435068	2.556736
-1395.292860	16.017144	2.566733
-1393.573609	10.910732	2.576730
-1391.590336	10.781335	2.586726
-1389.555505	6.767518	2.596723
-1387.709982	14.777233	2.606720
-1386.000296	10.944941	2.616717
-1383.858695	11.919107	2.626714
-1382.061828	14.724712	2.636710
-1380.034591	5.427584	2.646707
-1378.345595	12.426616	2.656704
-1376.697974	7.956924	2.666701
-1374.616903	14.530048	2.676698
-1372.585340	12.242491	2.686694
-1370.832391	6.426519	2.696691
-1369.246724	5.966070	2.706688
-1367.142162	6.330415	2.716685
-1365.310044	13.265495	2.726682
-1363.050129	10.685610	2.736678
-1361.303912	10.407879	2.746675
-1359.720634	4.020678	2.756672
-1357.766594	10.080489	2.766669
-1355.675704	2.260504	2.776666
-1354.249447	12.489388	2.786662
-1352.292839	11.139075	2.796659
-1350.358176	9.023360	2.806656
-1348.411536	13.136018	2.816653
-1346.395248	15.180239	2.826650
-1344.281578	7.200305	2.836646
-1342.677499	10.992029	2.846643
-1341.117966	9.310566	2.856640
-1338.962897	11.741510	2.866637
-1337.121626	12.743269	2.876634
-1335.081832	12.300146	2.886630
-1333.385089	14.578681	2.896627
-1331.477334	12.310977	2.906624
-1329.553321	12.222696	2.916621
-1327.616778	17.530630	2.926618
-1325.929197	13.160359	2.936614
-1323.798495	10.323311	2.946611
-1321.866628	10.685341	2.956608
-1320.236447	7.006343	2.966605
-1318.104108	14.007089	2.976602
-1316.412520	11.061920	2.986598
-1314.776618	9.777183	2.996595
-1312.596978	1.229371	3.006592
-1310.616816	4.132004	3.016589
-1308.806341	3.754030	3.026586
-1307.123396	9.228881	3.036582
-1305.582295	6.945678	3.046579
-1303.325524	10.781377	3.056576
-1301.308937	9.833597	3.066573
-1299.400235	5.661629	3.076570
-1297.734964	7.683131	3.086566
-1295.698373	2.123381	3.096563
-1293.640276	6.627178	3.106560
-1292.207076	8.641620	3.116557
-1290.152101	10.660752	3.126554
-1288.157169	7.550214	3.136550
-1286.359315	12.187249	3.146547
-1284.495472	14.254346	3.156544
-1282.504753	6.710967	3.166541
-1280.944846	14.130199	3.176538
-1278.924852	11.006183	3.186534
-1276.933399	1.268040	3.196531
-1275.266130	6.807001	3.206528
-1273.272402	10.752721	3.216525
-1271.226164	14.312686	3.226522
-1269.688297	13.951531	3.236518
-1267.655357	13.403779	3.246515
-1265.493178	8.217095	3.256512
-1264.042201	13.005976	3.266509
-1262.126123	11.918005	3.276506
-1260.067253	12.444491	3.286502
-1258.165723	12.795641	3.296499
-1256.296322	10.736234	3.306496
-1254.744575	15.193217	3.316493
-1252.582983	11.236592	3.326490
-1250.723104	17.644719	3.336486
-1249.014248	9.409132	3.346483
-1246.642261	2.172649	3.356480
-1245.280497	13.403475	3.366477
-1243.261424	17.425692	3.376474
-1241.407992	13.114197	3.386470
-1239.535081	9.772183	3.396467
-1237.475888	7.941356	3.406464
-1235.580755	11.201862	3.416461
-1233.646502	6.376933	3.426458
-1232.068265	7.657703	3.436454
-1230.425253	8.242870	3.446451
-1227.947032	12.286356	3.456448
-1226.154441	7.953032	3.466445
-1224.834718	13.811327	3.476442
-1222.477850	14.350157	3.486438
-1220.480240	2.740085	3.496435
-1218.826094	8.608021	3.506432
-1217.026006	15.036796	3.516429
-1214.906157	4.682908	3.526426
-1213.437052	10.913606	3.536422
-1211.304174	8.924173	3.546419
-1209.237131	14.176594	3.556416
-1207.670554	10.452586	3.566413
-1205.879915	13.174070	3.576410
-1203.801970	21.532010	3.586406
-1201.949245	15.528086	3.596403
-1199.923361	18.822963	3.606400
-1198.087056	10.988579	3.616397
-1196.395240	16.264740	3.626394
-1194.510358	17.736461	3.636390
-1192.482059	16.336916	3.646387
-1190.484354	12.618141	3.656384
-1188.870404	9.344444	3.666381
-1186.850993	13.024038	3.676378
-1185.238489	20.539135	3.686374
-1183.202081	19.266191	3.696371
-1181.196697	4.137133	3.706368
-1179.409311	22.109664	3.716365
-1177.673708	16.249230	3.726362
-1175.712086	22.484834	3.736358
-1173.852388	17.512409	3.746355
-1171.847634	18.184997	3.756352
-1169.948434	14.363583	3.766349
-1168.356892	22.295718	3.776346
-1166.086410	17.668085	3.786342
-1164.343166	13.912679	3.796339
-1162.630431	18.648697	3.806336
-1160.734335	16.087742	3.816333
-1158.560863	12.443499	3.826330
-1157.202354	15.453628	3.836326
-1154.881949	8.599677	3.846323
-1153.137232	11.379075	3.856320
-1151.285117	8.656224	3.866317
-1149.267584	17.323870	3.876314
-1147.102873	21.164986	3.886310
-1145.647139	14.749372	3.896307
-1144.089053	16.570251	3.906304
-1142.060253	19.312102	3.916301
-1140.132823	14.837270	3.926298
-1137.936789	21.422234	3.936294
-1136.109100	23.147883	3.946291
-1134.438169	12.599042	3.956288
-1132.796442	18.301673	3.966285
-1130.622351	14.456837	3.976282
-1128.742553	19.046158	3.986278
-1126.668318	17.917206	3.996275
-1124.974133	6.450476	4.006272
-1123.057816	11.900769	4.016269
-1121.345931	10.253496	4.026266
-1119.192035	15.368954	4.036262
-1117.501449	18.040202	4.046259
-1115.641356	15.000322	4.056256
-1113.515987	4.983515	4.066253
-1111.706336	10.202996	4.076250
-1110.090925	13.571514	4.086246
-1108.064114	10.411815	4.096243
-1106.472932	13.994205	4.106240
-1104.184117	12.548324	4.116237
-1102.613907	21.164424	4.126234
-1100.588200	16.204969	4.136230
-1098.865434	13.164966	4.146227
-1096.634119	16.157083	4.156224
-1094.925840	9.551105	4.166221
-1093.231346	11.675449	4.176218
-1091.207172	17.801652	4.186214
-1088.940131	18.073945	4.196211
-1087.517093	4.923306	4.206208
-1085.770093	9.328649	4.216205
-1083.311454	10.830254	4.226202
-1082.033912	7.305714	4.236198
-1079.976724	11.235142	4.246195
-1078.323577	9.257834	4.256192
-1076.239426	11.441434	4.266189
-1074.415467	7.993698	4.276186
-1072.365573	19.506144	4.286182
-1070.439777	14.257969	4.296179
-1068.782599	20.993933	4.306176
-1066.885839	9.829558	4.316173
-1064.925970	20.145402	4.326170
-1063.011210	7.402416	4.336166
-1061.209705	10.221747	4.346163
-1059.181642	17.340481	4.356160
-1057.164580	5.812674	4.366157
-1055.852615	20.045186	4.376154
-1053.817868	11.070778	4.386150
-1051.710522	16.533210	4.396147
-1049.894329	10.759444	4.406144
-1048.019119	9.507664	4.416141
-1046.153892	6.350179	4.426138
-1044.090032	15.698913	4.436134
-1042.689664	7.176498	4.446131
-1040.618703	7.072846	4.456128
-1038.563283	11.054699	4.466125
-1036.630397	4.385995	4.476122
-1034.786708	10.945312	4.486118
-1033.127515	6.807142	4.496115
-1031.302343	1.253002	4.506112
-1029.626139	10.439547	4.516109
-1027.423698	6.604479	4.526106
-1025.480476	13.809443	4.536102
-1023.735633	10.597021	4.546099
-1021.594219	11.560502	4.556096
-1019.973722	11.427866	4.566093
-1017.987662	11.232027	4.576090
-1016.229914	8.142280	4.586086
-1014.258776	22.105193	4.596083
-1012.080954	12.065863	4.606080
-1010.548053	8.213161	4.616077
-1008.876532	10.279665	4.626074
-1006.751115	12.687248	4.636070
-1004.944018	9.480672	4.646067
-1003.038598	13.491285	4.656064
-1001.143971	4.619854	4.666061
-999.283045	5.375590	4.676058
-997.541873	9.497735	4.686054
-995.430141	8.530263	4.696051
-993.455598	11.732488	4.706048
-991.538851	8.606277	4.716045
-989.891615	7.588363	4.726042
-988.334733	15.395128	4.736038
-986.174827	9.997478	4.746035
-984.260677	12.195720	4.756032
-982.220207	13.385373	4.766029
-980.567313	6.422025	4.776026
-978.751733	6.793465	4.786022
-976.877709	8.949183	4.796019
-974.919703	7.144237	4.806016
-972.871378	2.765464	4.816013
-971.032736	9.851414	4.826010
-969.243535	6.470891	4.836006
-967.230006	6.141233	4.846003
-965.713172	10.376644	4.856000
-963.700015	8.255004	4.865997
-961.500000	12.286434	4.875994
-960.078286	4.540622	4.885990
-957.732332	12.101230	4.895987
-955.851862	3.745237	4.905984
-954.471009	3.087302	4.915981
-952.418232	7.110707	4.925978
-950.537985	5.315059	4.935974
-948.496238	1.739436	4.945971
-946.782880	10.015401	4.955968
-944.868671	-2.833194	4.965965
-943.113735	13.311649	4.975962
-940.996250	6.232984	4.985958
-939.145805	14.453881	4.995955
-937.341708	-1.045436	5.005952
-935.277495	-0.498991	5.015949
-933.748511	12.765774	5.025946
-931.767222	1.112734	5.035942
-929.734502	10.453926	5.045939
-928.127119	16.116417	5.055936
-926.362320	10.349378	5.065933
-924.352985	13.751357	5.075930
-922.325673	11.936951	5.085926
-920.333661	9.943460	5.095923
-918.461124	19.333965	5.105920
-916.608792	6.886840	5.115917
-914.820609	11.104162	5.125914
-912.712960	11.102122	5.135910
-911.087162	18.492151	5.145907
-909.127359	5.748384	5.155904
-907.398445	12.023015	5.165901
-905.444167	7.736699	5.175898
-903.535948	6.132398	5.185894
-901.717657	13.848485	5.195891
-900.139386	5.556637	5.205888
-897.960047	12.076616	5.215885
-896.146607	11.393760	5.225882
-893.990659	8.281485	5.235878
-892.594603	11.257352	5.245875
-890.217001	5.744456	5.255872
-888.434355	6.707002	5.265869
-886.552933	4.576490	5.275866
-885.297146	11.398872	5.285862
-883.032713	10.269723	5.295859
-880.678830	6.773720	5.305856
-878.874482	8.029635	5.315853
-877.308856	8.338488	5.325850
-875.514984	6.000936	5.335846
-873.708005	5.825956	5.345843
-871.618395	2.444843	5.355840
-869.868019	7.514532	5.365837
-867.757159	3.785825	5.375834
-866.007649	7.805690	5.385830
-864.245862	6.695341	5.395827
-862.159974	7.970995	5.405824
-860.521373	6.722453	5.415821
-858.461482	12.061607	5.425818
-856.591425	9.506632	5.435814
-854.853411	9.194275	5.445811
-853.001338	4.655928	5.455808
-851.099608	6.755216	5.465805
-849.143890	11.376847	5.475802
-847.516698	6.907610	5.485798
-845.387051	8.258385	5.495795
-843.189516	11.852974	5.505792
-841.806889	15.263639	5.515789
-839.648298	8.330059	5.525786
-837.900373	15.342210	5.535782
-836.103292	8.990618	5.545779
-834.197578	10.326677	5.555776
-832.003837	10.190951	5.565773
-830.334471	5.678669	5.575770
-828.474761	8.436778	5.585766
-826.673872	8.734897	5.595763
-824.877770	11.436864	5.605760
-822.963175	4.458622	5.615757
-821.056797	8.753437	5.625754
-819.338844	0.481940	5.635750
-817.242816	9.506814	5.645747
-815.126931	4.383183	5.655744
-813.563251	8.836993	5.665741
-811.497957	1.040487	5.675738
-809.826354	6.988050	5.685734
-808.066846	1.964023	5.695731
-805.933296	6.961461	5.705728
-804.133319	0.574696	5.715725
-802.108555	5.543738	5.725722
-800.318030	12.337538	5.735718
-798.799709	5.147928	5.745715
-796.775337	12.063820	5.755712
-794.634768	6.715214	5.765709
-792.846062	9.094714	5.775706
-791.097556	5.210841	5.785702
-788.916069	2.778239	5.795699
-787.231961	15.893597	5.805696
-785.380660	5.467713	5.815693
-783.501204	6.193819	5.825690
-781.807131	7.988473	5.835686
-779.880403	14.163697	5.845683
-777.828889	6.078900	5.855680
-775.955825	5.661334	5.865677
-774.095397	7.320459	5.875674
-772.447020	5.209916	5.885670
-770.470941	4.048017	5.895667
-768.319636	5.106463	5.905664
-766.387382	-4.113431	5.915661
-764.760376	6.751663	5.925658
-763.023676	4.230706	5.935654
-760.983049	8.163074	5.945651
-758.873418	5.380416	5.955648
-757.170758	4.440644	5.965645
-755.345887	13.943117	5.975642
-753.297293	7.215079	5.985638
-751.564380	5.779438	5.995635
-749.923972	0.294502	6.005632
-747.655260	6.130892	6.015629
-745.915231	2.587869	6.025626
-744.291185	8.557295	6.035622
-742.258801	4.654928	6.045619
-740.428026	4.315198	6.055616
-738.270283	4.947920	6.065613
-736.535492	10.757552	6.075610
-734.627732	7.595085	6.085606
-732.933180	2.317815	6.095603
-731.091278	3.660998	6.105600
-729.113797	3.795185	6.115597
-726.975974	3.114299	6.125594
-725.220040	4.019661	6.135590
-723.543931	7.314024	6.145587
-721.551689	2.379174	6.155584
-719.627361	6.244904	6.165581
-717.962835	5.191258	6.175578
-716.075727	10.509211	6.185574
-714.232352	11.214298	6.195571
-711.886484	11.164895	6.205568
-710.175576	3.573517	6.215565
-708.422565	12.929625	6.225562
-706.430520	7.429571	6.235558
-704.679996	16.962919	6.245555
-702.787106	7.706722	6.255552
-700.762834	7.317155	6.265549
-699.062378	7.228803	6.275546
-697.359815	10.095813	6.285542
-695.077701	14.172805	6.295539
-693.414343	11.706246	6.305536
-691.769607	14.252513	6.315533
-689.592332	8.557087	6.325530
-687.744570	8.089951	6.335526
-685.976621	6.288770	6.345523
-684.097836	11.486506	6.355520
-682.167688	8.615755	6.365517
-680.161408	4.183942	6.375514
-678.427685	5.478140	6.385510
-676.775756	10.873180	6.395507
-674.738726	11.349991	6.405504
-672.571188	8.616573	6.415501
-670.659783	9.947121	6.425498
-669.174279	13.234088	6.435494
-667.089998	9.579270	6.445491
-665.341021	18.610809	6.455488
-663.655915	18.030739	6.465485
-661.462936	17.404255	6.475482
-659.701645	5.448672	6.485478
-657.804212	14.784905	6.495475
-655.504226	19.771687	6.505472
-654.018182	15.168814	6.515469
-652.300797	11.171591	6.525466
-650.283651	10.562159	6.535462
-648.266397	14.732043	6.545459
-646.559303	14.211627	6.555456
-644.714736	8.518876	6.565453
-642.651598	10.589390	6.575450
-640.725746	9.061424	6.585446
-639.045425	8.884755	6.595443
-637.267060	7.007736	6.605440
-635.271751	4.363447	6.615437
-633.251519	8.051302	6.625434
-631.495832	7.621025	6.635430
-629.728212	11.172408	6.645427
-627.770850	6.246361	6.655424
-625.774320	8.095434	6.665421
-624.238709	9.672371	6.675418
-622.046099	10.631197	6.685414
-620.251282	4.987464	6.695411
-618.328756	10.235108	6.705408
-616.519467	1.099697	6.715405
-614.438453	11.038197	6.725402
-613.206002	4.696445	6.735398
-610.803550	8.620087	6.745395
-608.960857	10.219024	6.755392
-607.115767	2.108921	6.765389
-605.089618	1.179152	6.775386
-603.448542	8.551184	6.785382
-601.425061	5.632429	6.795379
-599.675019	4.628358	6.805376
-597.724631	9.743677	6.815373
-595.810507	17.222093	6.825370
-594.124136	6.326909	6.835366
-591.894067	11.285451	6.845363
-590.203408	14.778110	6.855360
-588.372901	4.693564	6.865357
-586.613114	8.778321	6.875354
-584.765326	10.531195	6.885350
-582.512158	11.339862	6.895347
-580.812648	15.074266	6.905344
-578.951897	9.554233	6.915341
-577.272749	5.042134	6.925338
-574.987393	13.588597	6.935334
-573.287336	11.749396	6.945331
-571.680100	12.258641	6.955328
-569.314006	14.918701	6.965325
-567.496070	13.316455	6.975322
-566.353327	8.921629	6.985318
-563.871671	6.799687	6.995315
-561.879454	14.248289	7.005312
-560.108693	-0.189196	7.015309
-558.343911	4.262667	7.025306
-556.719884	8.997537	7.035302
-554.723412	5.271580	7.045299
-552.413533	9.105865	7.055296
-550.715775	6.307075	7.065293
-548.924330	12.185175	7.075290
-546.878599	8.692926	7.085286
-545.611878	12.629116	7.095283
-543.524483	14.654793	7.105280
-541.246394	4.517730	7.115277
-539.337379	7.552401	7.125274
-537.701591	8.301838	7.135270
-535.919191	6.121099	7.145267
-534.090885	7.889756	7.155264
-532.156380	9.200938	7.165261
-530.219127	6.390749	7.175258
-527.992999	1.868679	7.185254
-526.414956	7.060902	7.195251
-524.663353	7.693957	7.205248
-522.724273	8.410749	7.215245
-521.058195	5.223893	7.225242
-519.063321	5.985459	7.235238
-516.883338	12.889388	7.245235
-515.136815	5.497702	7.255232
-513.344707	9.902608	7.265229
-511.377174	3.284023	7.275226
-509.222298	9.236732	7.285222
-507.892050	8.113467	7.295219
-506.101291	7.366637	7.305216
-504.037270	15.165392	7.315213
-501.925954	6.471274	7.325210
-499.852121	6.853939	7.335206
-498.299761	15.965966	7.345203
-496.636167	5.999715	7.355200
-494.559500	16.916371	7.365197
-492.558735	3.252164	7.375194
-490.699465	10.489964	7.385190
-488.746228	12.582905	7.395187
-487.017547	8.306104	7.405184
-485.168829	12.053063	7.415181
-483.090383	4.632069	7.425178
-481.410348	9.252263	7.435174
-479.740333	8.262638	7.445171
-477.707514	10.080780	7.455168
-475.781637	6.151429	7.465165
-473.759066	6.441255	7.475162
-472.042412	8.440944	7.485158
-470.057689	4.911136	7.495155
-468.294341	2.392446	7.505152
-466.598516	14.009406	7.515149
-464.481835	6.692843	7.525146
-462.456652	11.870545	7.535142
-460.837180	10.647433	7.545139
-458.881697	12.476363	7.555136
-456.947188	11.825030	7.565133
-454.829198	7.666073	7.575130
-453.246373	4.527294	7.585126
-451.630403	8.786699	7.595123
-449.403389	9.887030	7.605120
-447.676169	0.046436	7.615117
-445.946370	5.937619	7.625114
-443.827848	8.599448	7.635110
-441.778431	8.185559	7.645107
-440.255039	5.889940	7.655104
-438.216505	2.446299	7.665101
-436.163791	15.555196	7.675098
-434.392431	5.276518	7.685094
-432.748534	6.796816	7.695091
-430.861634	1.670600	7.705088
-428.848463	5.018721	7.715085
-426.794564	5.530945	7.725082
-424.860841	10.476977	7.735078
-423.434191	10.449912	7.745075
-421.775296	12.743065	7.755072
-419.171686	10.237070	7.765069
-417.466201	8.202905	7.775066
-415.876943	5.819417	7.785062
-413.742015	8.886011	7.795059
-411.996269	18.271952	7.805056
-410.138422	13.502483	7.815053
-408.068230	0.810907	7.825050
-406.609267	12.165747	7.835046
-404.500824	13.919774	7.845043
-402.373283	18.659620	7.855040
-400.495949	13.992833	7.865037
-399.242259	12.897640	7.875034
-397.028801	15.072262	7.885030
-395.252290	8.834780	7.895027
-393.336910	10.420702	7.905024
-391.024580	10.043821	7.915021
-389.289556	10.400157	7.925018
-387.807622	15.468886	7.935014
-385.654496	14.961119	7.945011
-383.745060	18.414264	7.955008
-381.889442	13.960953	7.965005
-379.900643	11.264225	7.975002
-378.288927	9.879779	7.984998
-376.128200	11.581274	7.994995
-374.454893	2.769303	8.004992
-372.829070	9.539229	8.014989
-371.131932	10.046887	8.024986
-368.631479	7.229003	8.034982
-366.768611	8.057562	8.044979
-365.334694	13.934476	8.054976
-362.965171	7.359183	8.064973
-361.359514	9.345098	8.074970
-359.423849	6.708975	8.084966
-357.563121	15.885555	8.094963
-355.624042	13.067315	8.104960
-353.475886	12.320376	8.114957
-351.752985	18.323264	8.124954
-350.484652	10.472779	8.134950
-348.129647	11.592244	8.144947
-346.340319	9.025282	8.154944
-344.525658	14.710374	8.164941
-342.685557	10.095362	8.174938
-340.703792	7.933460	8.184934
-338.479753	6.636013	8.194931
-337.031901	12.723873	8.204928
-334.869915	6.207002	8.214925
-333.233021	9.223712	8.224922
-331.239096	9.706121	8.234918
-329.228745	6.197595	8.244915
-327.577020	10.152968	8.254912
-325.855578	6.625833	8.264909
-323.684770	1.743311	8.274906
-321.601156	5.149751	8.284902
-320.307540	1.141462	8.294899
-318.291404	7.520704	8.304896
-316.168993	8.699437	8.314893
-314.349183	12.132211	8.324890
-312.632333	3.564372	8.334886
-310.635528	11.203517	8.344883
-308.820429	15.761230	8.354880
-306.888057	16.851892	8.364877
-305.187391	8.420845	8.374874
-303.017456	9.064649	8.384870
-301.431724	6.797056	8.394867
-299.446758	14.237583	8.404864
-297.356285	9.071070	8.414861
-295.529966	7.950834	8.424858
-293.729190	3.861597	8.434854
-291.929152	11.969527	8.444851
-290.360031	11.766645	8.454848
-288.285779	12.998879	8.464845
-285.948042	13.781697	8.474842
-284.334978	13.357073	8.484838
-282.546614	6.225693	8.494835
-280.611182	9.409516	8.504832
-278.788146	12.394973	8.514829
-277.073197	14.780333	8.524826
-274.800147	12.044631	8.534822
-273.323450	7.411891	8.544819
-271.199970	10.540443	8.554816
-269.199531	11.192387	8.564813
-267.197964	13.861994	8.574810
-265.910999	6.027522	8.584807
-263.785192	2.134313	8.594803
-261.805138	12.984515	8.604800
-259.825158	5.587307	8.614797
-258.180070	-1.143825	8.624794
-256.451887	11.053918	8.634791
-254.423589	10.335672	8.644787
-252.352812	7.886481	8.654784
-250.732060	8.719041	8.664781
-248.905353	8.007714	8.674778
-246.613761	2.469679	8.684775
-244.885758	10.267048	8.694771
-243.071864	9.456721	8.704768
-241.051435	16.069031	8.714765
-239.626839	6.275282	8.724762
-237.824598	10.959837	8.734759
-235.680092	13.797705	8.744755
-233.611325	6.255296	8.754752
-231.661147	9.070501	8.764749
-229.802411	10.558231	8.774746
-228.245250	8.749970	8.784743
-226.116038	16.589110	8.794739
-224.482720	23.427429	8.804736
-222.546198	22.592808	8.814733
-220.652834	18.454105	8.824730
-218.543605	15.026197	8.834727
-216.762945	16.029043	8.844723
-214.862618	14.971264	8.854720
-212.818277	8.114856	8.864717
-211.135221	12.272152	8.874714
-209.301123	3.660402	8.884711
-207.521590	9.018060	8.894707
-205.697481	10.708699	8.904704
-203.574387	5.053912	8.914701
-201.754894	8.911551	8.924698
-200.086470	3.536167	8.934695
-197.899392	7.881447	8.944691
-196.274328	8.122844	8.954688
-194.277743	7.769701	8.964685
-192.420875	6.759926	8.974682
-190.607513	4.184504	8.984679
-188.502248	3.815600	8.994675
-186.861455	7.412829	9.004672
-185.026413	1.571929	9.014669
-183.069490	5.096605	9.024666
-181.283267	4.546523	9.034663
-179.680847	5.031539	9.044659
-177.469337	4.803580	9.054656
-175.465603	0.195734	9.064653
-173.652939	6.402321	9.074650
-171.664339	0.254300	9.084647
-169.869010	2.109028	9.094643
-168.223388	9.798030	9.104640
-166.106674	4.911641	9.114637
-164.172614	1.756465	9.124634
-162.422446	10.791386	9.134631
-160.505361	5.194771	9.144627
-158.695064	7.936045	9.154624
-156.789395	9.893173	9.164621
-155.138546	14.826158	9.174618
-152.825117	10.636265	9.184615
-150.976909	8.906342	9.194611
-149.497212	10.453041	9.204608
-147.644927	9.987176	9.214605
-145.450284	7.892510	9.224602
-143.427810	6.341623	9.234599
-141.958463	4.048494	9.244595
-139.868990	1.779567	9.254592
-137.932782	4.557606	9.264589
-136.428911	11.462430	9.274586
-134.146463	-0.557045	9.284583
-132.289448	3.195189	9.294579
-130.777985	2.381099	9.304576
-129.066593	4.520824	9.314573
-126.702106	-2.629747	9.324570
-124.524499	1.968158	9.334567
-123.182903	6.847880	9.344563
-121.347780	7.155281	9.354560
-119.145410	8.763526	9.364557
-117.552836	6.899159	9.374554
-115.248113	9.537893	9.384551
-113.710324	9.674853	9.394547
-111.716402	5.447559	9.404544
-109.664700	10.772922	9.414541
-108.156544	9.223601	9.424538
-106.125892	12.128701	9.434535
-104.268632	7.514280	9.444531
-102.544785	15.882416	9.454528
-100.656712	5.203226	9.464525
-98.679592	11.993096	9.474522
-96.552696	8.131429	9.484519
-94.940645	16.490568	9.494515
-92.977508	6.508336	9.504512
-91.320027	9.990870	9.514509
-89.122315	13.283004	9.524506
-87.176553	3.957220	9.534503
-85.488266	13.711009	9.544499
-83.759619	9.039755	9.554496
-81.797183	10.204748	9.564493
-79.615331	15.651477	9.574490
-77.955893	7.825554	9.584487
-76.097547	5.858812	9.594483
-74.669597	7.224345	9.604480
-72.518344	12.518070	9.614477
-70.423060	6.815724	9.624474
-68.530577	6.130353	9.634471
-66.924467	5.582248	9.644467
-64.621523	11.042828	9.654464
-63.103847	6.918392	9.664461
-61.084517	12.064232	9.674458
-59.339663	11.590310	9.684455
-57.492159	11.704737	9.694451
-55.428370	13.527777	9.704448
-53.539723	14.068265	9.714445
-51.512151	16.782856	9.724442
-49.792440	17.727657	9.734439
-48.245295	14.687976	9.744435
-46.181825	14.758484	9.754432
-44.445292	11.214919	9.764429
-42.228167	13.330870	9.774426
-40.262174	21.112549	9.784423
-38.586135	22.075378	9.794419
-36.905151	13.120275	9.804416
-34.849297	16.397198	9.814413
-33.010955	12.477407	9.824410
-31.104159	14.282883	9.834407
-29.068627	9.152193	9.844403
-27.245800	11.653155	9.854400
-25.441431	13.887071	9.864397
-23.578588	17.300580	9.874394
-22.037613	6.867858	9.884391
-19.976504	11.141826	9.894387
-17.914717	10.748427	9.904384
-16.101046	8.918327	9.914381
-14.171698	12.578597	9.924378
-12.473920	13.075354	9.934375
-10.365422	9.706157	9.944371
-8.645937	5.664822	9.954368
-6.610703	10.118188	9.964365
-4.782170	10.597252	9.974362
-3.341707	28.608885	9.984359
-2.139695	57.524677	9.994355
-0.715876	103.258545	10.004352
0.000000	136.569518	10.009357
0.923305	179.125035	10.014362
1.659701	199.121198	10.019367
1.841468	230.581727	10.024371
2.561083	246.540573	10.029376
2.859891	270.131047	10.034381
2.802846	279.071943	10.039386
3.052282	281.687807	10.044391
2.901315	292.942846	10.049395
3.262993	299.869464	10.054400
3.580408	327.199104	10.059405
3.412429	323.706314	10.064410
3.765634	323.825129	10.069415
3.601451	331.772337	10.074419
3.679255	324.279101	10.079424
3.651805	341.181950	10.084429
3.557157	334.645027	10.089434
3.944403	342.130551	10.094439
3.720573	339.756823	10.099443
3.745619	348.344051	10.104448
4.131393	348.236901	10.109453
3.964097	348.620088	10.114458
3.952518	350.071249	10.119463
3.763570	369.753210	10.124467
4.401887	370.141934	10.129472
4.420682	385.744374	10.134477
4.480257	397.276566	10.139482
4.575390	389.315336	10.144487
4.117028	368.978329	10.149491
4.471852	380.155910	10.154496
4.322762	388.564360	10.159501
4.155370	398.916940	10.164506
4.603879	384.807650	10.169511
4.433018	397.958262	10.174515
4.618099	396.162690	10.179520
4.690972	401.052294	10.184525
4.631907	398.316388	10.189530
4.881586	399.341108	10.194535
4.578456	413.963614	10.199539
4.888264	404.932086	10.204544
4.611841	403.648515	10.209549
4.633467	412.505982	10.214554
4.873866	404.258225	10.219559
4.838662	418.174108	10.224563
5.257046	431.292262	10.229568
4.916244	426.854042	10.234573
5.217323	445.786167	10.239578
5.223733	444.542632	10.244583
5.343299	449.910503	10.249587
5.276706	449.984318	10.254592
5.551437	453.578613	10.259597
5.616855	455.028541	10.264602
5.719339	427.335450	10.269607
5.300231	427.337763	10.274611
5.405044	429.271832	10.279616
5.449872	441.042952	10.284621
5.278902	455.586071	10.289626
5.911203	452.821876	10.294631
5.694112	469.703085	10.299635
5.812309	459.954617	10.304640
5.564278	461.087116	10.309645
5.737638	466.000138	10.314650
5.899516	460.065632	10.319655
5.720861	466.602283	10.324659
5.954996	466.621822	10.329664
5.906529	466.248049	10.334669
6.008869	473.157771	10.339674
5.966309	469.972944	10.344679
5.869611	467.768150	10.349683
5.910859	473.911761	10.354688
5.874238	488.745719	10.359693
5.935092	492.199098	10.364698
6.283848	489.245160	10.369703
6.383090	514.358077	10.374707
6.390179	512.086259	10.379712
6.465452	503.517856	10.384717
6.399118	522.846154	10.389722
6.345612	509.229979	10.394727
6.383380	520.647477	10.399731
6.369225	514.949185	10.404736
6.392327	511.747567	10.409741
6.140821	524.283533	10.414746
6.637949	516.340114	10.419751
6.596149	539.020264	10.424755
6.735254	536.891386	10.429760
6.966491	563.408897	10.434765
6.730807	563.022406	10.439770
7.047389	559.698271	10.444775
6.802137	567.669578	10.449779
7.234166	562.578187	10.454784
7.151849	560.686475	10.459789
7.132512	573.891925	10.464794
7.071821	565.021898	10.469799
6.782170	559.212992	10.474803
6.948949	571.644431	10.479808
7.106098	571.649443	10.484813
7.239055	567.783739	10.489818
7.621655	555.309058	10.494823
7.143789	568.190251	10.499827
7.120415	561.725435	10.504832
7.248296	577.831076	10.509837
7.073789	591.589572	10.514842
7.561082	591.185531	10.519847
7.548678	604.938684	10.524851
7.641883	603.586673	10.529856
7.650916	609.421667	10.534861
7.712519	612.971150	10.539866
7.557503	599.651781	10.544871
7.119158	607.914107	10.549875
7.819953	624.188613	10.554880
8.001614	637.406215	10.559885
8.013390	648.908384	10.564890
8.068667	647.305374	10.569895
7.878884	647.367301	10.574899
8.149646	653.297760	10.579904
8.224911	648.427250	10.584909
8.250521	651.250774	10.589914
8.430192	642.922682	10.594919
8.202120	655.559102	10.599923
8.486327	652.172301	10.604928
8.629606	654.775205	10.609933
8.359483	654.985566	10.614938
8.648804	649.992602	10.619943
8.416679	661.401220	10.624947
8.317046	657.498476	10.629952
8.220688	654.774777	10.634957
8.545194	659.099203	10.639962
8.808643	657.693224	10.644967
8.347938	666.670360	10.649971
8.297582	660.561467	10.654976
8.796944	673.807275	10.659981
8.679224	688.712720	10.664986
9.191255	685.221763	10.669991
9.272723	697.969696	10.674995
9.193849	690.859234	10.680000
9.114379	694.475394	10.685005
8.714357	698.699356	10.690010
9.130571	695.475994	10.695015
9.246270	704.253979	10.700019
9.020298	707.565501	10.705024
9.239487	699.538582	10.710029
8.962088	702.175480	10.715034
9.206587	700.009267	10.720039
9.129582	708.486829	10.725043
9.266896	702.934615	10.730048
9.057219	712.259673	10.735053
8.997795	727.256785	10.740058
9.294899	727.665255	10.745063
9.312043	734.719580	10.750067
8.925737	746.405173	10.755072
9.261608	748.248813	10.760077
9.439936	760.378947	10.765082
9.953271	759.828821	10.770087
9.424034	779.305414	10.775091
9.494289	778.341830	10.780096
9.800216	783.804680	10.785101
9.910065	775.657963	10.790106
10.192138	766.914491	10.795111
9.717355	781.250927	10.800115
9.676484	789.013133	10.805120
10.034087	791.091435	10.810125
10.180158	811.572124	10.815130
10.083318	814.487751	10.820135
10.300914	817.473076	10.825139
10.348227	804.605378	10.830144
10.313852	823.403844	10.835149
10.121557	834.634353	10.840154
10.295406	825.305702	10.845159
10.467915	816.781531	10.850163
10.322505	833.113977	10.855168
10.602706	835.803885	10.860173
10.444993	827.794436	10.865178
10.589712	822.078567	10.870183
10.318517	834.960145	10.875187
10.705265	824.810622	10.880192
10.397700	841.219405	10.885197
10.401650	842.475746	10.890202
10.897666	852.207157	10.895207
10.875102	853.109753	10.900211
10.727338	847.218172	10.905216
10.779973	844.708797	10.910221
10.881191	847.184402	10.915226
10.930619	848.305753	10.920231
10.775051	865.291150	10.925235
11.101096	867.294071	10.930240
11.173393	884.115408	10.935245
11.237238	892.867084	10.940250
11.487126	888.683016	10.945255
11.633997	898.127943	10.950259
11.452202	898.358911	10.955264
11.703963	886.425224	10.960269
11.345822	895.950702	10.965274
11.734474	890.290517	10.970279
11.694115	903.417616	10.975283
11.377753	887.714078	10.980288
11.653751	893.091855	10.985293
11.451638	905.686504	10.990298
11.761143	890.998064	10.995303
11.346119	893.377820	11.000307
11.491011	892.312436	11.005312
11.681256	898.672164	11.010317
11.667766	900.562087	11.015322
12.093565	915.988211	11.020327
11.605813	927.858868	11.025331
11.819127	928.739615	11.030336
12.255434	927.017449	11.035341
12.271059	936.372946	11.040346
12.201480	931.140659	11.045351
12.045597	933.863873	11.050355
12.155676	931.512482	11.055360
12.297283	934.197707	11.060365
12.237728	930.971333	11.065370
12.691581	929.683196	11.070375
12.393733	941.187673	11.075379
12.362246	931.048016	11.080384
12.744987	933.119176	11.085389
12.303686	938.464723	11.090394
12.583690	929.180577	11.095399
12.475923	942.509279	11.100403
12.696932	940.329431	11.105408
12.923613	965.170482	11.110413
12.819833	967.546338	11.115418
13.038349	969.143790	11.120423
12.995094	986.658632	11.125427
13.047636	958.500972	11.130432
13.200831	954.683979	11.135437
12.747294	945.409591	11.140442
12.747861	955.473995	11.145447
13.164929	973.082557	11.150451
13.178470	970.858524	11.155456
13.211460	972.326293	11.160461
12.860705	981.708719	11.165466
13.307069	973.350515	11.170471
13.202649	976.694751	11.175475
12.948258	970.249255	11.180480
13.125518	979.091705	11.185485
13.100902	984.331381	11.190490
13.213261	995.718430	11.195495
13.521451	1006.363813	11.200499
13.465726	1018.209788	11.205504
13.536989	1023.091975	11.210509
13.260985	1022.372846	11.215514
13.782448	1013.215717	11.220519
13.416530	1021.007815	11.225523
13.444186	1020.732275	11.230528
13.660643	1014.397743	11.235533
13.886737	1031.535351	11.240538
14.221783	1044.474961	11.245543
13.946937	1055.507489	11.250547
14.106432	1043.373918	11.255552
14.458184	1043.283234	11.260557
14.145978	1059.342908	11.265562
14.392045	1041.305412	11.270567
14.198415	1047.182370	11.275571
14.212078	1050.914654	11.280576
14.329227	1048.905904	11.285581
14.123552	1057.066713	11.290586
14.641933	1050.127323	11.295591
14.353957	1046.666113	11.300595
14.253724	1036.297643	11.305600
14.227275	1051.682504	11.310605
14.250760	1057.726691	11.315610
14.875062	1049.955094	11.320615
14.450982	1056.215754	11.325619
14.520479	1051.492692	11.330624
14.552816	1052.722445	11.335629
14.312168	1053.694533	11.340634
14.801594	1057.469208	11.345639
14.621472	1082.176644	11.350643
14.776733	1081.372953	11.355648
15.157015	1085.953549	11.360653
15.008017	1079.467538	11.365658
15.134459	1075.661089	11.370663
14.942517	1081.433708	11.375667
14.917475	1083.633014	11.380672
14.981218	1088.857056	11.385677
14.726832	1093.450575	11.390682
15.078382	1088.755054	11.395687
14.787063	1091.586636	11.400691
15.529253	1107.839317	11.405696
15.569081	1121.053174	11.410701
15.324569	1118.051810	11.415706
15.473034	1111.579841	11.420711
15.548372	1120.115348	11.425715
15.705441	1112.888194	11.430720
15.812484	1132.334733	11.435725
15.707193	1119.801769	11.440730
15.806030	1118.522932	11.445735
15.553001	1119.829749	11.450739
15.630500	1115.264668	11.455744
16.006490	1116.527925	11.460749
15.641314	1118.273691	11.465754
15.590054	1113.528868	11.470759
15.609873	1118.987017	11.475763
15.967591	1119.688618	11.480768
15.982404	1115.537251	11.485773
15.665979	1125.702799	11.490778
16.308268	1137.357107	11.495783
16.162237	1149.708045	11.500787
16.185638	1150.967619	11.505792
16.224054	1142.986638	11.510797
16.094843	1151.958506	11.515802
16.233070	1143.807056	11.520807
16.110956	1145.711184	11.525811
16.167420	1154.596664	11.530816
16.462408	1141.042587	11.535821
16.687514	1151.087082	11.540826
16.301812	1145.857830	11.545831
16.457192	1154.702301	11.550835
16.438367	1162.218329	11.555840
16.742433	1165.614151	11.560845
16.527300	1195.466866	11.565850
17.045112	1184.493485	11.570855
16.915947	1189.710485	11.575859
16.829138	1187.245371	11.580864
17.179524	1180.638658	11.585869
17.038709	1180.172358	11.590874
17.210080	1179.525371	11.595879
17.069925	1179.289211	11.600883
17.151418	1184.639772	11.605888
16.971358	1184.685956	11.610893
16.728701	1187.467214	11.615898
17.218806	1185.315375	11.620903
17.394602	1180.420767	11.625907
17.302227	1192.528208	11.630912
17.403763	1187.161297	11.635917
17.395575	1190.843485	11.640922
17.632486	1168.265475	11.645927
17.035374	1189.830373	11.650931
17.420480	1187.111784	11.655936
17.355365	1184.936536	11.660941
17.225486	1217.026104	11.665946
17.495815	1215.046516	11.670951
17.819935	1218.764020	11.675955
17.980531	1213.565883	11.680960
18.223617	1220.934505	11.685965
18.191924	1218.473211	11.690970
18.249087	1215.247081	11.695975
17.869615	1207.941450	11.700979
18.063072	1198.396536	11.705984
18.045286	1215.391904	11.710989
17.986196	1216.368160	11.715994
18.282538	1214.277186	11.720999
18.345594	1215.632947	11.726003
18.461059	1208.812945	11.731008
18.346688	1202.666724	11.736013
18.255296	1196.091044	11.741018
18.362620	1194.236812	11.746023
18.179311	1209.028667	11.751027
18.383163	1219.349425	11.756032
18.872629	1210.804431	11.761037
18.483605	1226.565868	11.766042
18.578394	1215.456501	11.771047
18.129485	1231.071369	11.776051
18.537915	1223.722063	11.781056
18.777021	1229.754007	11.786061
18.669883	1229.842178	11.791066
18.746645	1225.168366	11.796071
18.354900	1220.490432	11.801075
18.425558	1229.977695	11.806080
18.789454	1226.242147	11.811085
18.733148	1230.368855	11.816090
18.587179	1253.675467	11.821095
18.848847	1252.542543	11.826099
19.045131	1246.083389	11.831104
19.169911	1264.451744	11.836109
18.876606	1256.768051	11.841114
19.336507	1254.949041	11.846119
19.288861	1263.149417	11.851123
19.325671	1269.883882	11.856128
19.423906	1260.923423	11.861133
19.329909	1254.609919	11.866138
19.368517	1258.618989	11.871143
19.286600	1264.706884	11.876147
19.685289	1254.927337	11.881152
19.672257	1254.894837	11.886157
19.370290	1256.649462	11.891162
19.640368	1258.741795	11.896167
19.505605	1261.382849	11.901171
19.870717	1270.547193	11.906176
20.023072	1270.470965	11.911181
19.897190	1269.481861	11.916186
19.875295	1271.824204	11.921191
19.894437	1266.027261	11.926195
20.099315	1262.517351	11.931200
19.937906	1268.685738	11.936205
20.008796	1277.822895	11.941210
20.609761	1280.889101	11.946215
19.942773	1281.806197	11.951219
20.086395	1278.995215	11.956224
20.134800	1282.900222	11.961229
20.494600	1284.150308	11.966234
20.749646	1282.001253	11.971239
20.290777	1290.590527	11.976243
20.865367	1274.668761	11.981248
20.413035	1270.896227	11.986253
20.272612	1267.373579	11.991258
20.806026	1278.223737	11.996263
20.616190	1280.793150	12.001267
20.591310	1275.376982	12.006272
21.121612	1279.889556	12.011277
20.777903	1272.423639	12.016282
20.743676	1256.606886	12.021287
20.393671	1274.647264	12.026291
20.618949	1261.107349	12.031296
20.484142	1250.304249	12.036301
20.574331	1275.642288	12.041306
20.933257	1284.359751	12.046311
20.825141	1281.013305	12.051315
20.682791	1263.217271	12.056320
20.550589	1263.205356	12.061325
20.618744	1255.607518	12.066330
20.999756	1277.530644	12.071335
20.923143	1264.526179	12.076339
20.658901	1260.699992	12.081344
20.864298	1256.404640	12.086349
20.440356	1256.286286	12.091354
20.375342	1265.008276	12.096359
20.284969	1261.799360	12.101363
20.243062	1276.040425	12.106368
20.598752	1293.343762	12.111373
20.610762	1293.441315	12.116378
20.944343	1279.150788	12.121383
20.701991	1294.969332	12.126387
20.935183	1285.403830	12.131392
20.767349	1286.569332	12.136397
20.607608	1292.666497	12.141402
20.895920	1289.242625	12.146407
21.102417	1286.964112	12.151411
20.979691	1278.735933	12.156416
20.796137	1269.329957	12.161421
20.499365	1260.754217	12.166426
20.816659	1246.576711	12.171431
20.466778	1265.657896	12.176435
20.479036	1269.064016	12.181440
20.919939	1257.965647	12.186445
20.470297	1262.397964	12.191450
20.782149	1254.010592	12.196455
20.736011	1266.064985	12.201459
20.402383	1253.151991	12.206464
20.548589	1257.479805	12.211469
20.454718	1255.886326	12.216474
21.102054	1274.668108	12.221479
20.740937	1278.840294	12.226483
20.519431	1266.757846	12.231488
21.118624	1262.686700	12.236493
20.399688	1274.760099	12.241498
20.420692	1266.143131	12.246503
20.859092	1261.293347	12.251507
20.824069	1263.875914	12.256512
20.740690	1261.123221	12.261517
20.786853	1273.337948	12.266522
21.070245	1266.314508	12.271527
20.939524	1273.884713	12.276531
20.789257	1271.767190	12.281536
20.705663	1261.971520	12.286541
20.476421	1276.349704	12.291546
20.448660	1274.069131	12.296551
20.536508	1273.479619	12.301555
20.348531	1273.232161	12.306560
20.894650	1262.375638	12.311565
20.628855	1275.641538	12.316570
20.958282	1266.417107	12.321575
20.750916	1268.527245	12.326579
20.630587	1273.861142	12.331584
21.016341	1268.948787	12.336589
20.671521	1282.817107	12.341594
20.875963	1279.968037	12.346599
21.104964	1275.525405	12.351603
20.786030	1277.191270	12.356608
21.054568	1276.708562	12.361613
20.839697	1282.820825	12.366618
20.814290	1267.149318	12.371623
20.770728	1276.528667	12.376627
20.614481	1265.050854	12.381632
20.478131	1259.043738	12.386637
20.690357	1268.962631	12.391642
21.279514	1272.729342	12.396647
21.101729	1255.811066	12.401651
20.689316	1238.223725	12.406656
20.706405	1258.873860	12.411661
20.707794	1246.815803	12.416666
20.855223	1228.412169	12.421671
20.395985	1246.156107	12.426675
20.426663	1242.532054	12.431680
20.625017	1239.081539	12.436685
20.422605	1250.880135	12.441690
20.536978	1243.260739	12.446695
20.587228	1267.706230	12.451699
20.773329	1274.222911	12.456704
20.779440	1264.837152	12.461709
20.518778	1261.727941	12.466714
20.872506	1261.124407	12.471719
20.981009	1258.714865	12.476723
20.688847	1265.260515	12.481728
20.746441	1246.645672	12.486733
20.514066	1251.032292	12.491738
20.871920	1252.774718	12.496743
20.505144	1261.838164	12.501747
20.833385	1253.181661	12.506752
21.008851	1254.935830	12.511757
20.700586	1256.402863	12.516762
20.848132	1261.157840	12.521767
20.890859	1258.927531	12.526771
20.495362	1256.240393	12.531776
20.679809	1249.297401	12.536781
20.671325	1258.339968	12.541786
20.784901	1251.928699	12.546791
20.656908	1263.961451	12.551795
20.906192	1261.947366	12.556800
20.556692	1265.712399	12.561805
20.169899	1263.348740	12.566810
20.670648	1258.597827	12.571815
20.801273	1254.601420	12.576819
20.539315	1263.282279	12.581824
20.682713	1260.811974	12.586829
20.657108	1258.948973	12.591834
21.065640	1260.054081	12.596839
20.698339	1271.139368	12.601843
20.747857	1265.988893	12.606848
20.929893	1262.700256	12.611853
20.649930	1264.271590	12.616858
20.640067	1274.175445	12.621863
20.721771	1255.875304	12.626867
20.746378	1252.851488	12.631872
20.863425	1259.603114	12.636877
20.887268	1265.107987	12.641882
20.885943	1262.074111	12.646887
20.702955	1262.865119	12.651891
20.564452	1261.346570	12.656896
20.904840	1253.937135	12.661901
20.877941	1261.404037	12.666906
20.937631	1266.633521	12.671911
20.912857	1264.740422	12.676915
20.595547	1243.069174	12.681920
20.744114	1231.538037	12.686925
20.744111	1240.011511	12.691930
20.615111	1226.551791	12.696935
20.332093	1243.807128	12.701939
20.332273	1252.003023	12.706944
20.714396	1256.274283	12.711949
20.642247	1261.070610	12.716954
21.039758	1260.450631	12.721959
20.999806	1260.676326	12.726963
20.902749	1251.627167	12.731968
20.749013	1237.572112	12.736973
20.669416	1238.914357	12.741978
20.609410	1235.137605	12.746983
20.502068	1237.987180	12.751987
20.412459	1232.393687	12.756992
20.949641	1241.218315	12.761997
20.598520	1259.720921	12.767002
20.613893	1248.583194	12.772007
20.505605	1247.954001	12.777011
20.652531	1261.016856	12.782016
20.686504	1270.822249	12.787021
20.982137	1268.587871	12.792026
20.989096	1260.372135	12.797031
20.633441	1246.443900	12.802035
19.967573	1243.208505	12.807040
20.852633	1254.278535	12.812045
20.708364	1270.094024	12.817050
21.043843	1265.208613	12.822055
21.072324	1250.175110	12.827059
20.766702	1255.007098	12.832064
20.937090	1233.750106	12.837069
20.594816	1249.903099	12.842074
20.420635	1245.947427	12.847079
20.479643	1239.928084	12.852083
20.607589	1249.816249	12.857088
20.488737	1244.315729	12.862093
20.250390	1250.382835	12.867098
20.856639	1267.549978	12.872103
20.993009	1274.500389	12.877107
20.848942	1259.305155	12.882112
20.765030	1247.535106	12.887117
20.836963	1255.091902	12.892122
21.085236	1244.784395	12.897127
20.993872	1246.760904	12.902131
20.655043	1250.323949	12.907136
20.812987	1244.236782	12.912141
20.683027	1248.197039	12.917146
20.650242	1246.161712	12.922151
20.993209	1253.266826	12.927155
20.819941	1249.154882	12.932160
20.900348	1250.014269	12.937165
20.684052	1259.514204	12.942170
20.899507	1242.435444	12.947175
20.980023	1255.409534	12.952179
20.968295	1247.259867	12.957184
20.898631	1216.358249	12.962189
20.510108	1230.123098	12.967194
20.527877	1219.038630	12.972199
20.703436	1219.422347	12.977203
20.700022	1222.010904	12.982208
20.703438	1219.163947	12.987213
20.462738	1226.338489	12.992218
20.676624	1231.286310	12.997223
20.824003	1233.838201	13.002227
20.807460	1235.440059	13.007232
20.984476	1218.878414	13.012237
20.653321	1225.553274	13.017242
20.685138	1217.746778	13.022247
20.637015	1218.069974	13.027251
20.775681	1227.682012	13.032256
20.802210	1220.519784	13.037261
20.619400	1227.182022	13.042266
21.079733	1216.120010	13.047271
20.677306	1219.019803	13.052275
20.672639	1217.364788	13.057280
20.796170	1221.661514	13.062285
20.798711	1222.596400	13.067290
20.855920	1214.390022	13.072295
20.926273	1224.340975	13.077299
20.919879	1221.620167	13.082304
20.379197	1208.016385	13.087309
20.156017	1218.122968	13.092314
20.664463	1212.762111	13.097319
20.776902	1220.355007	13.102323
20.603079	1223.226223	13.107328
20.404759	1221.457010	13.112333
20.591258	1227.371183	13.117338
20.644364	1222.925082	13.122343
20.504626	1219.593156	13.127347
20.921815	1227.230492	13.132352
20.945094	1221.306746	13.137357
20.286974	1230.892905	13.142362
20.745371	1221.534385	13.147367
20.801555	1222.250970	13.152371
20.650417	1226.365994	13.157376
20.528791	1220.156264	13.162381
20.425456	1225.533167	13.167386
20.556930	1225.163790	13.172391
20.417225	1219.325968	13.177395
20.546301	1238.554660	13.182400
20.864446	1241.511419	13.187405
20.455602	1245.536660	13.192410
20.654294	1252.628514	13.197415
20.996098	1260.266853	13.202419
20.953144	1242.932828	13.207424
20.935785	1227.349971	13.212429
20.777298	1235.232104	13.217434
20.769416	1215.113800	13.222439
20.915961	1220.157519	13.227443
20.566670	1227.291032	13.232448
21.002623	1226.149235	13.237453
20.347662	1230.947045	13.242458
20.800448	1217.809294	13.247463
20.799044	1224.721730	13.252467
20.649453	1219.125192	13.257472
20.709772	1219.716533	13.262477
20.906765	1225.696843	13.267482
20.869563	1226.668032	13.272487
20.601654	1230.855301	13.277491
20.565496	1232.701573	13.282496
20.750708	1225.827859	13.287501
20.497243	1238.834704	13.292506
20.763476	1225.876519	13.297511
20.850573	1236.250606	13.302515
20.702176	1226.388022	13.307520
20.887867	1227.385162	13.312525
20.598970	1231.441732	13.317530
21.002515	1226.591211	13.322535
20.933535	1215.531621	13.327539
20.933576	1233.763709	13.332544
21.024483	1224.853328	13.337549
20.587457	1218.769603	13.342554
20.909374	1211.096618	13.347559
20.807000	1197.823498	13.352563
20.749911	1200.679243	13.357568
20.695688	1199.192992	13.362573
20.790676	1202.522820	13.367578
21.025037	1197.327116	13.372583
20.381637	1196.890515	13.377587
20.568802	1201.795278	13.382592
20.567415	1191.488204	13.387597
20.556904	1199.916020	13.392602
20.839210	1200.678543	13.397607
20.729592	1202.064998	13.402611
20.526949	1204.388849	13.407616
20.700084	1201.076412	13.412621
20.343443	1203.382247	13.417626
20.537926	1200.883303	13.422631
20.667564	1210.663934	13.427635
20.730721	1227.834072	13.432640
20.716606	1224.529419	13.437645
20.633342	1237.567465	13.442650
21.034132	1229.523906	13.447655
20.792645	1213.327078	13.452659
20.661313	1216.910637	13.457664
20.727424	1209.953422	13.462669
20.666729	1205.992276	13.467674
20.657669	1202.396649	13.472679
20.581658	1206.903402	13.477683
20.656357	1210.269586	13.482688
21.008578	1204.580397	13.487693
20.553436	1219.803569	13.492698
20.615837	1203.730176	13.497703
20.469475	1206.751556	13.502707
20.455936	1198.889223	13.507712
20.562236	1217.011297	13.512717
20.521729	1235.271931	13.517722
20.811448	1244.453015	13.522727
20.946522	1237.401204	13.527731
20.844716	1239.232715	13.532736
20.730325	1209.778069	13.537741
20.657053	1226.099450	13.542746
20.814912	1210.316767	13.547751
20.555211	1220.489104	13.552755
20.558491	1211.707830	13.557760
20.664054	1212.523777	13.562765
20.476123	1218.347851	13.567770
20.745572	1229.993893	13.572775
20.918323	1229.718862	13.577779
20.512334	1233.103372	13.582784
20.984206	1210.699140	13.587789
20.527537	1222.095124	13.592794
20.337153	1219.354775	13.597799
20.544207	1217.459400	13.602803
20.791757	1236.494143	13.607808
20.962603	1230.509007	13.612813
20.765903	1227.512610	13.617818
20.843184	1209.771499	13.622823
20.626480	1213.750314	13.627827
20.636866	1216.308282	13.632832
20.548504	1219.877103	13.637837
20.354833	1220.889019	13.642842
20.659424	1233.327432	13.647847
20.615972	1237.628719	13.652851
20.935448	1244.707612	13.657856
20.917015	1235.664847	13.662861
20.683692	1226.749407	13.667866
20.533396	1220.993702	13.672871
20.483181	1214.662193	13.677875
20.368924	1232.903048	13.682880
20.907759	1229.398227	13.687885
20.901811	1248.107549	13.692890
20.653889	1234.293035	13.697895
20.466639	1230.487693	13.702899
20.707988	1241.723468	13.707904
20.838176	1243.301923	13.712909
20.656589	1238.286096	13.717914
20.706837	1241.854892	13.722919
21.034856	1238.448354	13.727923
20.740791	1226.997283	13.732928
21.004187	1226.936463	13.737933
20.664891	1228.752234	13.742938
20.849755	1217.492874	13.747943
20.861051	1223.584808	13.752947
20.824240	1217.822042	13.757952
20.712526	1213.788604	13.762957
20.516509	1230.635792	13.767962
20.484143	1218.139999	13.772967
20.794646	1225.305474	13.777971
20.496021	1226.906590	13.782976
20.887479	1218.262102	13.787981
20.818597	1225.475473	13.792986
20.739765	1220.746052	13.797991
20.592443	1214.168245	13.802995
20.923899	1228.889053	13.808000
21.284114	1218.458049	13.813005
20.815533	1230.705955	13.818010
20.598348	1228.044000	13.823015
20.915818	1220.969412	13.828019
20.744550	1219.968626	13.833024
20.629151	1216.606010	13.838029
20.450828	1227.522343	13.843034
20.541442	1220.285234	13.848039
20.713872	1225.409985	13.853043
20.799538	1218.299829	13.858048
21.019870	1219.622618	13.863053
20.653009	1227.586872	13.868058
20.598546	1225.234869	13.873063
20.657075	1215.028613	13.878067
20.849741	1222.652871	13.883072
20.772845	1221.130808	13.888077
20.517310	1224.992812	13.893082
20.939773	1224.638525	13.898087
20.755678	1220.965152	13.903091
20.747583	1202.398691	13.908096
20.807395	1186.563861	13.913101
20.433345	1190.682889	13.918106
20.251644	1203.034831	13.923111
20.479699	1207.393732	13.928115
20.278078	1222.907645	13.933120
20.368807	1230.232761	13.938125
20.267544	1226.330122	13.943130
20.434588	1229.788818	13.948135
20.591713	1229.855340	13.953139
20.496117	1230.875268	13.958144
20.427505	1225.398282	13.963149
20.295093	1239.215334	13.968154
20.792972	1248.637620	13.973159
21.157924	1243.310679	13.978163
20.800547	1238.132071	13.983168
20.732600	1239.016697	13.988173
20.694827	1229.800393	13.993178
21.007413	1232.582988	13.998183
20.687550	1230.744847	14.003187
20.415384	1231.557962	14.008192
20.833969	1225.501384	14.013210
20.567849	1236.584848	14.018227
20.485418	1232.730100	14.023245
20.806127	1229.344297	14.028263
20.735566	1229.555439	14.033280
20.665388	1234.087557	14.038298
20.572616	1227.525750	14.043315
20.826951	1230.379622	14.048333
20.664392	1234.004695	14.053351
20.549194	1257.747225	14.058368
20.892854	1250.212891	14.063386
20.573246	1265.161914	14.068403
20.668936	1263.381855	14.073421
20.814537	1269.281114	14.078439
20.593464	1258.662526	14.083456
20.484958	1267.366085	14.088474
20.807719	1260.870116	14.093491
20.862614	1259.650262	14.098509
20.788710	1263.701643	14.103527
20.495793	1274.960868	14.108544
20.977365	1278.972417	14.113562
20.855386	1295.838905	14.118579
20.971627	1294.772857	14.123597
21.316266	1302.907088	14.128615
21.322973	1290.172626	14.133632
21.552348	1297.771541	14.138650
20.834001	1303.129076	14.143667
20.850157	1301.803714	14.148685
21.255453	1296.434997	14.153703
21.253654	1292.913433	14.158720
21.611368	1292.263469	14.163738
21.580297	1293.891886	14.168755
21.413019	1281.389674	14.173773
21.568512	1271.077523	14.178791
21.194061	1277.242204	14.183808
21.229181	1261.884179	14.188826
21.220170	1269.289870	14.193843
20.995450	1277.670629	14.198861
21.385455	1277.095738	14.203879
21.249865	1298.658254	14.208896
21.344248	1296.409643	14.213914
21.510853	1306.011577	14.218931
21.300211	1294.287045	14.223949
21.767478	1290.575835	14.228967
21.746500	1307.539484	14.233984
21.486818	1283.138034	14.239002
21.439628	1288.364917	14.244019
21.321714	1302.746986	14.249037
21.841045	1302.228543	14.254055
21.341912	1302.525348	14.259072
21.544654	1300.250014	14.264090
21.734759	1309.772698	14.269107
21.526651	1305.233267	14.274125
21.817411	1300.675614	14.279143
21.642518	1299.711057	14.284160
21.507002	1305.236749	14.289178
21.469426	1305.695886	14.294195
21.849282	1298.449906	14.299213
22.113978	1295.409647	14.304231
21.387238	1308.580087	14.309248
21.595243	1297.104953	14.314266
21.540137	1304.525879	14.319283
21.692605	1298.796371	14.324301
21.510632	1293.859522	14.329319
21.466732	1294.101019	14.334336
21.487218	1300.915289	14.339354
21.335727	1301.244732	14.344371
21.647897	1321.825091	14.349389
21.942692	1325.855434	14.354407
21.455457	1332.623288	14.359424
21.790051	1330.254560	14.364442
22.049647	1327.591058	14.369459
21.860712	1334.426163	14.374477
21.990029	1328.248881	14.379495
22.089480	1333.022958	14.384512
22.287701	1330.249696	14.389530
22.315087	1344.986153	14.394547
21.858404	1334.861263	14.399565
22.105135	1330.865898	14.404583
21.942664	1336.804884	14.409600
22.204143	1328.838455	14.414618
22.040674	1331.389330	14.419635
22.137484	1337.714820	14.424653
22.386740	1338.467978	14.429671
22.468801	1332.840921	14.434688
22.202400	1333.319254	14.439706
22.350511	1332.966986	14.444723
22.374083	1341.231101	14.449741
22.560633	1340.216755	14.454759
22.098897	1335.297774	14.459776
22.393565	1333.397881	14.464794
22.567056	1333.793465	14.469811
22.400553	1328.690544	14.474829
22.724175	1341.723366	14.479847
22.520215	1338.246620	14.484864
22.734677	1328.017832	14.489882
22.306110	1345.118894	14.494899
22.210779	1344.882534	14.499917
22.448449	1328.891239	14.504935
22.121213	1348.041508	14.509952
22.450698	1338.714579	14.514970
22.718800	1331.739663	14.519987
22.485607	1335.803887	14.525005
22.856062	1344.029978	14.530023
22.603118	1337.594342	14.535040
22.561763	1338.878341	14.540058
22.783204	1338.901338	14.545075
22.616359	1335.541369	14.550093
22.904120	1330.631830	14.555111
22.593093	1328.896186	14.560128
22.446803	1327.469318	14.565146
22.743428	1337.305362	14.570163
22.457609	1339.027900	14.575181
22.830958	1333.068093	14.580199
22.667408	1343.090796	14.585216
22.813775	1336.808545	14.590234
22.842340	1341.183375	14.595251
22.633818	1337.266913	14.600269
22.905075	1334.088748	14.605287
22.877941	1335.876989	14.610304
22.707267	1340.768086	14.615322
22.533442	1332.057838	14.620339
22.803228	1353.159377	14.625357
23.006851	1363.027576	14.630375
23.023022	1367.805510	14.635392
23.103629	1370.506223	14.640410
23.345665	1365.051837	14.645427
22.952672	1351.525354	14.650445
23.177210	1333.381118	14.655463
23.098205	1346.383783	14.660480
22.931799	1360.734318	14.665498
23.392809	1367.737903	14.670515
23.264924	1366.599103	14.675533
22.962162	1341.314100	14.680551
23.151000	1352.759237	14.685568
23.229774	1359.461991	14.690586
23.168389	1353.118489	14.695603
23.441542	1376.470510	14.700621
23.770912	1356.297636	14.705639
23.184783	1341.389399	14.710656
23.015121	1336.170576	14.715674
23.178628	1351.695431	14.720691
23.320603	1359.418430	14.725709
23.604675	1371.126815	14.730727
23.520711	1359.791009	14.735744
23.501284	1362.153748	14.740762
23.677328	1358.684026	14.745779
23.055535	1356.159529	14.750797
23.256513	1350.436420	14.755815
23.458458	1371.424538	14.760832
23.151484	1367.221753	14.765850
23.510403	1373.329274	14.770867
23.386681	1376.907290	14.775885
23.612916	1369.668474	14.780903
23.646561	1374.921821	14.785920
23.798862	1369.450286	14.790938
24.090876	1367.901594	14.795955
23.616218	1381.327619	14.800973
23.788991	1368.113571	14.805991
23.755547	1372.111339	14.811008
23.316051	1371.465833	14.816026
23.760862	1357.689309	14.821043
23.432717	1367.187727	14.826061
23.816877	1363.227061	14.831079
23.724741	1372.849859	14.836096
23.816180	1361.589894	14.841114
23.602319	1358.410450	14.846131
23.341520	1361.423591	14.851149
23.527696	1368.327868	14.856167
23.760956	1378.620784	14.861184
23.629245	1401.653606	14.866202
24.142637	1392.997303	14.871219
24.046521	1395.174079	14.876237
24.353080	1385.064268	14.881255
24.273623	1393.851358	14.886272
24.289284	1374.900394	14.891290
24.373907	1371.517610	14.896307
24.285995	1361.263095	14.901325
24.286089	1356.098986	14.906343
24.257059	1359.534479	14.911360
24.017225	1363.856172	14.916378
24.194155	1360.269905	14.921395
23.952148	1364.209702	14.926413
24.128602	1358.894766	14.931431
23.769728	1364.721947	14.936448
23.797955	1373.284210	14.941466
24.316625	1379.907372	14.946483
24.293262	1387.008674	14.951501
24.471069	1378.418491	14.956519
24.411752	1382.417242	14.961536
24.624520	1396.809580	14.966554
24.604902	1378.635018	14.971571
24.488758	1375.628746	14.976589
24.328702	1358.304017	14.981607
24.447068	1376.074500	14.986624
24.235029	1362.781837	14.991642
24.468569	1372.653136	14.996659
24.443475	1394.627603	15.001677
24.406640	1393.961915	15.006695
24.811532	1384.322484	15.011712
24.580239	1400.202943	15.016730
24.392812	1383.920743	15.021747
24.455459	1397.909165	15.026765
24.783520	1389.523097	15.031783
24.523875	1394.459863	15.036800
24.667556	1397.148948	15.041818
24.919060	1374.902643	15.046835
24.712660	1394.717963	15.051853
24.698192	1390.790984	15.056871
24.946266	1389.667721	15.061888
24.954355	1389.540706	15.066906
25.094538	1385.280750	15.071923
24.661203	1402.244214	15.076941
24.853514	1386.381213	15.081959
24.798018	1394.388984	15.086976
24.802737	1393.243189	15.091994
24.666652	1384.924864	15.097011
24.567067	1402.157563	15.102029
24.746059	1389.323175	15.107047
24.885025	1389.356182	15.112064
24.670048	1387.866332	15.117082
24.594087	1390.131127	15.122099
24.708043	1392.530797	15.127117
24.842044	1406.212119	15.132135
24.932569	1422.064867	15.137152
24.847800	1422.973553	15.142170
25.578421	1419.632438	15.147187
25.402431	1421.548252	15.152205
25.222779	1424.111162	15.157223
25.375478	1432.740124	15.162240
25.359947	1420.622574	15.167258
25.344264	1398.934801	15.172275
24.979226	1403.071983	15.177293
25.217206	1408.668702	15.182311
25.558620	1415.579701	15.187328
25.301453	1424.108865	15.192346
25.385561	1414.157211	15.197363
25.235169	1406.689013	15.202381
25.292007	1424.579481	15.207399
25.594653	1415.502176	15.212416
25.739804	1418.415972	15.217434
25.315323	1407.261857	15.222451
25.292630	1421.921437	15.227469
25.800582	1415.392716	15.232487
25.797782	1425.638374	15.237504
25.403136	1402.354648	15.242522
25.562995	1408.711012	15.247539
25.443140	1422.352615	15.252557
25.395787	1419.248845	15.257575
25.673987	1426.383864	15.262592
25.535601	1421.551704	15.267610
25.669872	1412.773390	15.272627
25.515373	1429.904769	15.277645
25.913291	1424.710215	15.282663
25.950834	1419.156292	15.287680
25.708260	1417.824997	15.292698
25.760696	1421.558969	15.297715
25.827955	1422.435542	15.302733
25.572268	1416.470641	15.307751
25.857935	1415.969017	15.312768
25.790306	1417.859681	15.317786
25.712746	1407.844155	15.322803
25.706174	1418.905235	15.327821
25.571640	1411.911132	15.332839
25.858460	1412.112464	15.337856
25.569912	1436.335966	15.342874
25.925441	1429.213352	15.347891
25.895436	1437.800672	15.352909
26.163891	1449.903295	15.357927
26.458708	1447.791005	15.362944
26.248177	1448.136160	15.367962
26.396868	1442.012368	15.372979
26.233375	1442.142381	15.377997
26.303543	1441.061649	15.383015
26.634287	1429.842113	15.388032
26.210870	1420.745332	15.393050
26.068565	1425.524967	15.398067
26.457724	1414.001971	15.403085
26.159291	1416.448546	15.408103
26.040094	1424.192787	15.413120
26.222710	1424.247146	15.418138
26.477437	1435.098247	15.423155
26.421570	1448.569220	15.428173
26.223933	1450.203773	15.433191
26.606062	1444.432857	15.438208
26.354347	1449.599611	15.443226
26.496913	1455.206848	15.448243
26.740558	1442.423450	15.453261
26.603352	1444.375552	15.458279
26.848354	1443.012103	15.463296
26.542682	1442.949289	15.468314
26.873744	1447.175229	15.473331
26.513303	1423.514778	15.478349
26.405280	1433.929809	15.483367
26.515873	1425.501328	15.488384
26.594258	1448.724084	15.493402
26.708427	1441.002886	15.498419
26.466385	1456.015238	15.503437
26.651397	1447.538695	15.508455
26.773068	1450.503434	15.513472
26.934413	1448.484792	15.518490
26.940893	1445.894675	15.523507
26.694190	1448.366038	15.528525
26.560352	1455.016232	15.533543
27.015792	1452.102820	15.538560
27.092779	1452.941664	15.543578
26.828005	1450.940651	15.548595
27.054841	1442.798787	15.553613
26.739766	1447.182842	15.558631
26.879913	1449.104864	15.563648
26.904105	1457.656810	15.568666
26.705397	1453.562572	15.573683
26.811176	1463.454311	15.578701
27.016702	1481.475289	15.583719
27.367458	1480.365530	15.588736
27.114178	1476.874595	15.593754
27.406897	1474.268705	15.598771
27.267212	1484.877585	15.603789
27.469215	1486.185702	15.608807
27.605800	1472.680030	15.613824
27.387392	1477.607101	15.618842
27.576326	1452.164826	15.623859
27.222226	1449.520536	15.628877
27.011538	1457.450847	15.633895
27.229429	1451.838259	15.638912
27.406471	1473.815212	15.643930
27.469631	1477.228164	15.648947
27.523673	1480.979199	15.653965
27.254231	1478.700501	15.658983
27.384110	1471.679925	15.664000
27.578965	1474.017942	15.669018
27.440557	1477.790234	15.674035
27.554667	1473.836433	15.679053
27.434628	1480.404213	15.684071
27.993805	1472.228201	15.689088
27.613643	1482.118808	15.694106
27.775362	1473.410012	15.699123
27.993212	1472.760327	15.704141
27.585515	1474.142095	15.709159
27.933249	1467.811939	15.714176
27.636411	1472.737361	15.719194
27.709751	1472.977464	15.724211
28.006843	1473.548393	15.729229
27.763947	1472.698491	15.734247
27.805489	1472.113106	15.739264
27.765187	1463.224180	15.744282
27.357718	1472.837565	15.749299
27.645442	1463.098793	15.754317
27.801937	1472.106272	15.759335
27.834545	1480.156666	15.764352
27.934743	1500.956707	15.769370
28.110563	1500.285411	15.774387
27.883118	1495.626307	15.779405
27.661490	1498.079521	15.784423
27.860065	1496.007744	15.789440
28.358419	1490.559620	15.794458
28.012963	1498.093023	15.799475
28.285901	1491.158159	15.804493
28.124899	1497.310908	15.809511
28.238408	1488.142602	15.814528
27.999146	1491.586491	15.819546
27.998761	1493.272957	15.824563
28.124814	1492.049599	15.829581
28.000511	1507.527718	15.834599
28.256211	1515.685694	15.839616
28.491528	1524.100185	15.844634
28.329897	1520.179340	15.849651
28.799513	1512.948826	15.854669
28.681185	1512.020850	15.859687
29.114490	1507.128937	15.864704
28.744502	1504.049868	15.869722
28.736762	1480.127002	15.874739
29.107794	1482.605234	15.879757
28.805726	1479.524776	15.884775
28.854882	1482.104684	15.889792
28.797356	1485.835763	15.894810
28.998309	1489.964491	15.899827
29.216274	1481.794133	15.904845
28.973144	1489.871209	15.909863
28.928985	1477.025146	15.914880
29.085691	1488.164056	15.919898
28.637110	1489.006505	15.924915
29.034725	1483.060071	15.929933
28.786679	1487.559289	15.934951
28.792421	1478.736941	15.939968
28.929225	1475.927830	15.944986
28.824663	1483.545500	15.950003
28.873614	1472.960763	15.955021
28.846734	1464.562052	15.960039
29.238147	1482.713832	15.965056
28.620732	1484.544331	15.970074
28.783307	1483.115374	15.975091
29.283685	1472.155041	15.980109
29.124778	1477.582282	15.985127
29.021842	1479.061733	15.990144
29.394739	1473.814524	15.995162
29.022457	1477.885242	16.000179
29.242546	1481.197659	16.005197
28.858977	1481.542100	16.010215
29.250937	1484.164859	16.015232
29.152861	1488.081732	16.020250
29.077975	1487.488176	16.025267
29.310245	1488.270793	16.030285
29.130447	1521.674599	16.035303
29.263964	1506.695452	16.040320
29.549113	1509.440646	16.045338
29.553146	1506.882369	16.050355
29.539380	1519.042649	16.055373
29.599440	1516.127793	16.060391
29.850206	1510.939377	16.065408
29.561082	1518.871221	16.070426
29.367213	1523.366528	16.075443
29.682016	1515.484301	16.080461
29.276949	1521.447899	16.085479
29.565385	1517.988528	16.090496
29.786487	1512.416303	16.095514
29.698419	1512.194511	16.100531
29.817007	1502.682465	16.105549
29.817101	1510.994466	16.110567
30.108117	1503.627275	16.115584
30.187825	1510.145906	16.120602
29.915785	1508.119302	16.125619
30.069887	1512.180003	16.130637
29.884948	1520.295006	16.135655
29.979951	1512.215030	16.140672
29.958912	1514.567039	16.145690
30.006767	1519.119745	16.150707
30.314398	1509.855969	16.155725
30.137798	1518.811213	16.160743
30.325423	1503.933551	16.165760
30.308885	1503.140350	16.170778
29.943857	1519.493730	16.175795
30.224755	1515.206573	16.180813
30.196751	1523.211603	16.185831
30.459728	1515.449327	16.190848
30.518739	1506.774196	16.195866
30.452402	1517.728480	16.200883
30.464082	1502.359781	16.205901
30.103103	1485.625373	16.210919
30.220223	1488.139386	16.215936
30.210949	1502.068594	16.220954
30.566010	1510.374316	16.225971
30.263849	1493.954561	16.230989
30.255742	1513.466280	16.236007
30.264912	1509.250780	16.241024
30.407463	1506.311758	16.246042
30.336119	1513.826617	16.251059
30.584323	1507.622431	16.256077
30.174594	1515.744971	16.261095
30.162212	1502.530446	16.266112
30.458962	1509.753783	16.271130
30.450655	1536.919942	16.276147
30.709292	1538.184425	16.281165
30.949041	1533.765399	16.286183
30.868491	1530.726676	16.291200
31.186921	1534.506342	16.296218
30.802905	1523.270176	16.301235
30.620626	1513.875324	16.306253
30.835408	1528.907697	16.311271
30.927883	1535.687000	16.316288
31.306200	1538.162507	16.321306
30.825006	1536.951058	16.326323
31.031884	1522.306261	16.331341
30.960073	1530.529068	16.336359
30.518031	1538.604864	16.341376
30.844316	1535.383272	16.346394
30.851782	1534.974782	16.351411
31.082919	1542.378488	16.356429
30.971361	1543.442467	16.361447
30.909973	1537.098884	16.366464
31.216351	1535.860918	16.371482
30.962900	1542.420118	16.376499
31.755295	1532.515862	16.381517
31.535239	1533.803212	16.386535
31.323705	1539.331679	16.391552
31.324844	1535.032508	16.396570
31.391800	1541.273187	16.401587
31.317846	1527.014527	16.406605
31.448450	1540.954496	16.411623
31.585619	1527.794747	16.416640
31.699240	1533.161237	16.421658
31.557810	1531.705259	16.426675
31.830520	1539.829076	16.431693
31.537412	1525.613237	16.436711
31.614057	1544.126760	16.441728
31.612031	1528.697298	16.446746
31.484311	1535.870374	16.451763
31.375913	1532.147103	16.456781
31.374778	1543.545613	16.461799
31.515472	1559.348037	16.466816
32.024488	1557.368310	16.471834
31.421510	1570.382389	16.476851
31.905819	1555.605218	16.481869
32.037290	1568.231589	16.486887
32.040087	1560.196181	16.491904
32.239174	1563.483653	16.496922
31.902041	1563.292147	16.501939
32.224766	1556.892009	16.506957
32.095164	1557.115718	16.511975
32.133201	1565.519227	16.516992
32.383288	1555.240553	16.522010
32.059872	1552.641686	16.527027
32.106647	1545.354329	16.532045
32.449861	1542.214980	16.537063
31.887272	1544.261685	16.542080
32.093434	1545.405549	16.547098
32.227646	1555.104051	16.552115
32.318199	1548.868364	16.557133
32.335345	1559.521498	16.562151
32.429603	1557.474216	16.567168
32.479244	1547.070214	16.572186
32.172271	1564.886747	16.577203
32.074916	1554.230904	16.582221
32.319008	1565.286722	16.587239
32.364058	1552.037823	16.592256
32.438214	1549.819141	16.597274
32.069014	1561.458844	16.602291
32.567337	1557.305311	16.607309
32.656515	1549.479502	16.612327
32.369987	1552.243526	16.617344
32.717904	1541.980718	16.622362
32.759428	1556.126820	16.627379
32.700995	1539.177351	16.632397
32.557832	1551.372455	16.637415
32.746311	1557.257128	16.642432
32.849890	1555.788810	16.647450
32.867899	1559.009207	16.652467
32.785849	1566.816813	16.657485
33.122304	1569.020575	16.662503
32.706788	1569.974159	16.667520
33.432865	1558.881808	16.672538
33.131302	1563.597225	16.677555
32.895842	1550.240484	16.682573
33.071546	1546.080210	16.687591
33.033786	1552.938495	16.692608
33.060210	1551.984283	16.697626
32.962144	1568.133114	16.702643
33.138609	1572.619705	16.707661
33.537615	1567.036388	16.712679
32.951988	1577.027471	16.717696
33.425450	1570.118789	16.722714
33.320394	1573.580617	16.727731
33.387429	1562.549333	16.732749
33.699365	1562.701045	16.737767
33.408193	1561.473442	16.742784
33.584055	1561.974049	16.747802
33.388995	1562.138985	16.752819
33.389022	1555.850093	16.757837
33.399546	1560.608542	16.762855
33.412162	1567.100147	16.767872
33.895406	1562.524297	16.772890
33.812474	1564.316747	16.777907
33.535613	1572.032730	16.782925
33.986762	1563.405133	16.787943
33.485933	1549.049368	16.792960
33.742469	1555.958244	16.797978
33.855361	1564.883073	16.802995
33.726013	1573.295981	16.808013
33.668565	1553.628127	16.813031
33.502238	1570.289647	16.818048
33.564563	1562.719800	16.823066
33.761198	1567.277106	16.828083
33.352166	1574.329900	16.833101
33.631395	1566.454893	16.838119
33.675485	1571.813612	16.843136
33.707781	1571.762958	16.848154
33.516016	1587.763160	16.853171
33.987278	1596.442085	16.858189
34.422348	1590.126262	16.863207
33.925411	1596.823422	16.868224
34.387183	1592.930542	16.873242
34.584110	1589.694965	16.878259
34.600764	1598.643030	16.883277
34.567336	1595.263292	16.888295
34.316926	1586.178137	16.893312
34.302234	1576.462356	16.898330
34.391427	1588.216158	16.903347
34.110351	1598.641605	16.908365
34.607061	1594.494611	16.913383
34.343991	1602.140770	16.918400
34.646406	1597.118693	16.923418
34.464578	1600.510974	16.928435
34.447655	1596.625230	16.933453
34.716193	1585.351002	16.938471
34.649651	1597.839093	16.943488
34.739343	1600.261545	16.948506
34.913782	1593.120545	16.953523
34.796324	1598.218746	16.958541
35.012796	1583.746965	16.963559
34.904182	1602.398651	16.968576
35.022510	1578.586077	16.973594
34.623585	1573.995197	16.978611
34.654883	1582.808782	16.983629
34.885868	1596.578636	16.988647
34.877650	1602.782567	16.993664
34.946373	1590.420199	16.998682
34.723588	1597.061049	17.003699
34.836206	1597.826578	17.008717
35.145638	1589.525166	17.013735
34.704180	1600.371027	17.018752
34.832786	1591.615531	17.023770
34.586563	1599.461924	17.028787
34.820493	1597.744720	17.033805
35.150336	1611.199943	17.038823
35.078229	1611.291785	17.043840
35.329386	1623.903834	17.048858
35.436939	1616.417982	17.053875
35.495687	1627.745659	17.058893
35.533344	1622.024897	17.063911
35.500284	1625.437501	17.068928
35.594037	1616.807100	17.073946
35.666179	1615.192779	17.078963
35.307026	1611.595999	17.083981
35.725902	1617.571365	17.088999
35.842666	1610.831243	17.094016
35.821790	1608.034672	17.099034
35.487073	1591.915730	17.104051
35.428998	1605.052143	17.109069
35.828459	1604.914613	17.114087
35.411147	1618.377326	17.119104
35.270704	1619.095127	17.124122
35.713305	1611.176735	17.129139
35.470255	1624.015475	17.134157
35.660966	1606.922369	17.139175
35.664676	1628.132817	17.144192
35.848544	1617.732525	17.149210
35.445940	1615.036163	17.154227
35.687292	1638.829414	17.159245
36.215274	1642.441978	17.164263
35.952664	1653.061148	17.169280
36.044419	1641.333721	17.174298
36.290931	1637.707974	17.179315
35.885471	1640.561770	17.184333
36.238774	1633.178288	17.189351
36.243498	1632.024608	17.194368
36.606992	1641.055808	17.199386
36.818862	1624.984932	17.204403
36.483201	1647.047069	17.209421
36.935356	1627.109070	17.214439
36.479702	1617.800225	17.219456
36.107903	1610.082515	17.224474
36.640427	1611.715458	17.229491
36.664270	1634.275521	17.234509
36.843436	1613.849392	17.239527
36.480131	1606.737523	17.244544
36.393368	1600.855715	17.249562
36.632424	1610.977985	17.254579
36.704564	1632.646292	17.259597
37.050686	1633.695481	17.264615
36.722290	1622.695760	17.269632
36.360060	1620.081049	17.274650
36.770784	1618.810704	17.279667
36.716649	1634.551476	17.284685
36.748314	1642.809753	17.289703
36.755109	1642.193724	17.294720
36.891245	1636.732533	17.299738
36.866162	1632.959767	17.304755
36.566175	1638.950698	17.309773
36.816084	1626.504344	17.314791
36.894734	1634.632425	17.319808
36.895435	1646.925787	17.324826
37.285758	1639.813253	17.329843
36.910861	1650.261565	17.334861
37.340253	1655.014586	17.339879
37.406608	1664.620164	17.344896
37.155703	1652.599737	17.349914
37.101893	1648.246375	17.354931
36.803839	1664.784292	17.359949
37.362648	1656.001041	17.364967
37.597927	1666.948230	17.369984
37.222078	1667.812121	17.375002
37.196926	1658.017728	17.380019
37.586774	1665.102024	17.385037
37.516964	1661.712343	17.390055
37.415567	1670.650967	17.395072
37.257078	1669.303089	17.400090
37.859615	1660.427916	17.405107
37.354251	1668.847368	17.410125
37.489371	1660.026298	17.415143
37.293230	1671.621181	17.420160
37.861002	1677.440689	17.425178
38.413672	1680.415386	17.430195
37.852377	1678.011741	17.435213
37.841385	1666.365177	17.440231
38.210621	1672.828264	17.445248
38.091181	1667.448725	17.450266
38.157061	1644.693631	17.455283
37.938031	1661.563438	17.460301
38.157776	1643.366098	17.465319
38.070991	1639.966545	17.470336
37.908786	1657.725494	17.475354
38.183742	1673.492472	17.480371
38.243573	1683.182474	17.485389
38.347349	1680.196119	17.490407
38.511033	1683.231285	17.495424
38.338294	1678.969243	17.500442
38.210301	1674.295791	17.505459
38.369797	1688.577365	17.510477
38.791833	1678.752533	17.515495
38.666527	1677.358462	17.520512
38.432771	1674.882127	17.525530
38.759527	1679.552424	17.530547
39.049407	1673.934561	17.535565
38.766285	1640.889192	17.540583
38.610661	1648.675543	17.545600
38.529805	1637.516778	17.550618
38.471780	1634.647474	17.555635
38.396100	1648.725843	17.560653
38.813908	1667.361291	17.565671
38.740763	1667.797797	17.570688
38.848003	1668.141037	17.575706
39.035428	1660.935010	17.580723
39.058235	1675.263542	17.585741
39.502677	1669.474735	17.590759
39.169491	1676.751438	17.595776
38.959724	1675.907249	17.600794
39.368332	1663.152403	17.605811
39.208154	1654.559335	17.610829
39.209222	1644.243236	17.615847
39.062011	1640.507251	17.620864
39.023224	1634.218223	17.625882
39.472396	1637.190542	17.630899
39.059212	1648.057097	17.635917
39.153968	1658.738825	17.640935
39.178764	1651.676720	17.645952
39.353722	1662.134870	17.650970
39.378059	1669.246006	17.655987
39.461537	1662.710946	17.661005
39.505742	1661.771193	17.666023
39.292203	1672.767948	17.671040
39.330007	1660.699893	17.676058
39.482445	1668.523638	17.681075
39.246272	1673.382820	17.686093
39.351020	1668.925509	17.691111
39.656996	1667.102424	17.696128
39.547648	1689.311004	17.701146
39.800483	1683.466234	17.706163
39.883300	1695.085858	17.711181
39.409249	1702.608415	17.716199
39.744891	1691.367448	17.721216
39.613593	1708.852538	17.726234
39.807581	1700.280035	17.731251
39.930781	1704.622577	17.736269
39.599732	1711.109284	17.741287
39.813086	1696.472718	17.746304
39.686775	1722.328816	17.751322
40.512287	1718.686208	17.756339
40.624020	1735.503346	17.761357
40.382566	1720.181082	17.766375
40.179846	1703.756239	17.771392
40.287971	1724.814892	17.776410
40.469763	1715.119591	17.781427
40.562486	1727.657898	17.786445
40.601034	1705.885509	17.791463
40.133117	1705.335753	17.796480
39.815806	1705.708955	17.801498
40.556540	1725.150287	17.806515
40.627427	1721.766466	17.811533
40.567986	1725.941513	17.816551
40.729242	1726.534121	17.821568
40.576612	1722.429310	17.826586
40.537591	1726.295928	17.831603
40.387313	1721.078592	17.836621
40.646772	1712.550696	17.841639
40.807104	1719.443534	17.846656
41.024421	1726.984823	17.851674
40.929232	1710.586867	17.856691
40.892746	1714.287907	17.861709
40.687520	1722.486483	17.866727
40.876460	1722.789952	17.871744
41.041624	1735.840540	17.876762
41.542628	1747.280247	17.881779
41.417178	1746.100129	17.886797
41.178627	1737.403105	17.891815
41.094360	1731.410731	17.896832
41.248335	1730.783809	17.901850
41.532991	1725.737779	17.906867
41.409643	1727.498941	17.911885
41.554697	1715.884078	17.916903
41.509617	1717.903321	17.921920
41.409071	1709.621612	17.926938
41.538280	1718.337864	17.931955
41.489303	1710.334226	17.936973
41.437807	1719.623576	17.941991
41.910393	1716.537491	17.947008
41.548594	1723.049556	17.952026
41.747800	1704.125518	17.957043
41.337059	1717.406372	17.962061
41.183374	1741.854268	17.967079
41.818175	1734.353477	17.972096
41.862828	1744.989775	17.977114
41.516466	1737.914465	17.982131
41.689591	1747.479473	17.987149
41.790714	1749.742822	17.992167
41.612606	1747.482546	17.997184
41.550700	1745.590709	18.002202
42.156234	1762.834071	18.007219
42.124744	1781.019071	18.012237
42.198223	1779.833964	18.017255
42.555048	1778.166354	18.022272
42.320032	1776.363472	18.027290
42.182920	1767.121703	18.032307
42.288956	1765.618365	18.037325
42.640699	1770.424709	18.042343
42.452737	1756.138388	18.047360
42.360057	1750.639716	18.052378
42.586047	1769.549714	18.057395
42.487091	1763.756302	18.062413
42.442035	1779.215778	18.067431
42.541504	1769.283454	18.072448
42.654220	1769.912121	18.077466
42.891251	1769.643192	18.082483
42.650110	1763.641218	18.087501
42.567718	1765.833163	18.092519
42.916793	1762.431705	18.097536
42.986769	1762.879994	18.102554
42.950609	1766.085481	18.107571
43.059733	1752.552468	18.112589
43.117389	1761.865336	18.117607
43.182031	1755.693469	18.122624
43.130532	1752.735010	18.127642
43.091975	1753.446006	18.132659
43.158245	1754.609054	18.137677
42.931671	1768.194069	18.142695
43.309500	1749.406654	18.147712
43.158177	1764.146872	18.152730
42.761093	1760.403516	18.157747
42.965110	1758.697358	18.162765
43.051914	1765.504415	18.167783
43.552326	1760.699247	18.172800
43.318856	1754.101438	18.177818
43.228644	1760.788858	18.182835
43.520993	1758.796472	18.187853
43.442036	1758.233442	18.192871
43.710711	1754.130641	18.197888
43.439386	1757.103067	18.202906
43.490348	1771.658443	18.207923
43.660386	1758.949430	18.212941
43.485601	1766.353500	18.217959
43.616444	1788.527068	18.222976
43.606118	1790.572239	18.227994
43.678229	1796.362310	18.233011
43.634627	1794.915870	18.238029
43.757856	1791.868186	18.243047
44.198112	1783.869850	18.248064
44.004854	1794.756493	18.253082
43.964403	1784.860632	18.258099
44.157143	1787.990290	18.263117
44.073152	1793.828853	18.268135
44.401162	1784.366594	18.273152
44.272025	1781.417366	18.278170
44.456289	1781.462027	18.283187
44.247398	1779.279016	18.288205
44.073426	1786.675101	18.293223
44.262179	1798.296789	18.298240
44.126241	1784.823281	18.303258
44.335490	1796.021690	18.308275
44.665471	1805.629361	18.313293
44.691422	1810.295766	18.318311
44.961030	1815.808948	18.323328
44.795389	1789.752509	18.328346
44.759464	1784.024543	18.333363
45.078149	1769.091099	18.338381
44.652485	1778.010719	18.343399
44.937201	1771.660597	18.348416
44.958956	1776.558901	18.353434
44.680335	1773.429018	18.358451
45.104403	1767.907697	18.363469
44.668265	1776.769211	18.368487
45.168893	1786.349652	18.373504
45.263266	1802.519962	18.378522
45.000422	1797.539207	18.383539
45.079216	1795.656384	18.388557
45.139466	1809.617272	18.393575
45.245847	1811.269443	18.398592
45.161919	1809.659542	18.403610
45.121003	1811.494085	18.408627
45.401131	1810.872208	18.413645
45.338311	1810.361659	18.418663
45.181084	1816.889903	18.423680
45.136781	1815.279974	18.428698
44.913869	1808.608094	18.433715
45.099212	1809.470577	18.438733
44.868569	1826.764008	18.443751
45.284449	1832.425331	18.448768
45.416058	1831.385109	18.453786
45.361522	1833.026767	18.458803
45.517965	1821.315619	18.463821
45.643149	1837.363074	18.468839
45.679234	1848.730719	18.473856
45.933114	1854.796998	18.478874
45.929033	1853.507848	18.483891
46.246436	1860.124010	18.488909
45.997200	1851.675593	18.493927
46.216560	1856.134983	18.498944
46.329668	1850.046584	18.503962
46.105391	1856.467559	18.508979
46.260382	1848.184342	18.513997
46.103579	1852.842155	18.519015
46.358298	1861.315099	18.524032
46.410214	1846.246368	18.529050
46.373009	1855.934659	18.534067
46.714377	1845.847294	18.539085
46.366688	1860.367238	18.544103
46.360951	1846.882344	18.549120
46.618412	1848.751103	18.554138
46.391308	1860.679846	18.559155
46.742506	1846.724307	18.564173
46.612662	1848.519554	18.569191
46.463496	1855.084283	18.574208
46.574185	1848.985259	18.579226
46.200134	1848.311983	18.584243
46.884275	1853.084218	18.589261
46.846574	1868.426208	18.594279
46.837201	1880.053606	18.599296
47.023111	1882.511885	18.604314
46.872431	1876.666900	18.609331
46.963176	1875.055875	18.614349
47.191970	1877.476639	18.619367
47.547329	1875.600034	18.624384
47.185348	1882.364676	18.629402
47.574158	1869.012683	18.634419
47.493141	1862.989848	18.639437
47.269470	1862.363375	18.644455
47.494547	1871.643319	18.649472
47.621666	1870.057955	18.654490
47.200324	1871.191814	18.659507
47.304258	1870.428144	18.664525
47.400415	1870.420790	18.669543
47.222338	1866.876863	18.674560
47.571089	1877.463185	18.679578
47.421822	1862.124494	18.684595
47.861215	1859.127047	18.689613
47.511138	1872.359038	18.694631
47.857217	1884.544819	18.699648
48.493798	1881.747945	18.704666
48.087456	1884.656198	18.709683
48.135056	1856.522994	18.714701
48.304024	1867.498215	18.719719
48.069812	1863.236484	18.724736
48.066785	1864.025191	18.729754
47.642348	1877.198259	18.734771
48.182794	1858.321845	18.739789
47.899804	1880.180087	18.744807
48.220571	1891.509439	18.749824
48.450861	1894.117950	18.754842
48.104928	1899.844172	18.759859
48.447545	1896.446860	18.764877
48.412488	1905.331787	18.769895
48.335612	1901.610471	18.774912
48.347781	1894.076767	18.779930
48.158451	1897.779421	18.784947
48.132519	1889.162442	18.789965
48.383711	1904.211422	18.794983
48.649273	1921.992920	18.800000
48.606578	1920.395307	18.805018
48.581695	1923.665886	18.810035
48.753291	1928.209996	18.815053
48.983696	1926.970747	18.820071
49.031131	1921.142126	18.825088
49.238768	1915.190425	18.830106
48.656113	1927.926288	18.835123
49.494938	1918.900801	18.840141
49.285953	1924.200123	18.845159
49.287039	1922.431141	18.850176
49.620416	1910.983508	18.855194
49.471813	1920.367129	18.860211
49.282706	1916.377409	18.865229
49.430752	1913.719797	18.870247
49.757580	1914.646240	18.875264
49.721052	1917.180902	18.880282
49.447714	1917.059440	18.885299
49.580580	1909.220964	18.890317
49.461919	1923.473200	18.895335
49.362699	1921.748531	18.900352
49.596695	1922.419998	18.905370
49.089186	1920.544936	18.910387
49.526138	1923.705676	18.915405
49.585617	1941.288823	18.920423
49.736328	1948.072403	18.925440
49.965050	1938.356884	18.930458
49.785590	1952.831210	18.935475
50.168700	1942.000921	18.940493
50.029400	1947.089356	18.945511
49.815153	1954.233964	18.950528
50.077020	1946.986035	18.955546
50.357663	1943.148697	18.960563
50.348492	1954.470944	18.965581
50.290578	1948.975304	18.970599
50.219569	1944.939998	18.975616
50.659752	1945.660381	18.980634
50.330928	1953.637331	18.985651
50.541661	1935.646350	18.990669
50.531206	1942.786765	18.995687
50.609227	1940.854495	19.000704
50.633456	1935.879818	19.005722
50.608747	1953.589669	19.010739
50.821195	1961.182197	19.015757
50.752200	1976.150967	19.020775
51.017445	1980.942863	19.025792
51.360407	1968.457781	19.030810
51.040510	1956.779237	19.035827
51.020932	1937.307751	19.040845
51.208358	1932.576043	19.045863
50.941408	1937.474828	19.050880
50.922460	1931.752748	19.055898
51.059777	1952.705613	19.060915
51.093998	1966.899686	19.065933
51.290069	1973.576153	19.070951
51.307182	1973.255777	19.075968
51.542526	1960.863374	19.080986
51.395214	1969.512191	19.086003
51.458786	1962.516112	19.091021
51.464078	1966.627419	19.096039
51.335748	1963.670159	19.101056
51.517872	1955.945716	19.106074
51.436009	1957.327469	19.111091
51.263543	1952.625626	19.116109
51.631096	1951.893842	19.121127
51.890054	1958.861517	19.126144
51.845389	1957.796702	19.131162
51.633159	1959.428130	19.136179
52.095480	1979.302764	19.141197
51.791436	1981.585936	19.146215
51.836861	1994.733723	19.151232
52.040030	1985.755305	19.156250
51.923440	1994.416541	19.161267
52.094097	1986.913356	19.166285
52.205014	1986.602402	19.171303
52.263601	1983.483187	19.176320
52.562106	1988.124271	19.181338
52.343923	1985.296173	19.186355
52.152006	1986.782000	19.191373
52.509734	1997.265514	19.196391
52.216308	1988.360005	19.201408
52.550568	2002.543227	19.206426
52.671859	2008.570941	19.211443
52.692554	2007.725369	19.216461
52.986933	2011.267531	19.221479
52.668110	2010.207110	19.226496
52.851074	2007.338625	19.231514
52.613093	2011.225252	19.236531
52.724175	2010.665724	19.241549
52.835241	2007.679712	19.246567
52.711653	2006.112295	19.251584
52.863719	1999.820199	19.256602
52.938677	2004.981451	19.261619
53.282405	2020.751212	19.266637
53.474524	2018.716574	19.271655
53.558199	2013.121245	19.276672
53.375027	2005.030304	19.281690
53.478416	2001.423362	19.286707
53.407130	1996.580307	19.291725
53.594510	1993.148742	19.296743
53.118935	2004.131694	19.301760
53.455683	2013.322343	19.306778
53.971022	2022.720478	19.311795
54.007606	2024.757414	19.316813
53.910248	2026.333561	19.321831
53.561106	2017.294556	19.326848
54.035835	2023.280064	19.331866
54.027749	2028.057365	19.336883
54.014807	2030.389289	19.341901
54.082653	2025.497291	19.346919
53.759538	2043.189561	19.351936
53.704263	2026.341271	19.356954
54.411592	2022.996666	19.361971
54.260544	2025.048583	19.366989
54.424608	2022.636945	19.372007
54.051361	2031.738701	19.377024
54.212821	2019.792991	19.382042
54.286363	2023.424649	19.387059
54.247085	2023.998914	19.392077
54.295573	2021.479076	19.397095
53.950679	2024.381488	19.402112
54.525610	2036.617417	19.407130
54.579799	2051.191436	19.412147
54.887973	2062.020328	19.417165
54.858151	2058.070448	19.422183
54.583248	2060.302579	19.427200
54.593236	2049.948588	19.432218
54.935359	2051.001595	19.437235
54.787213	2057.231970	19.442253
55.137800	2051.587765	19.447271
54.802312	2053.714722	19.452288
54.814673	2055.694175	19.457306
55.015903	2066.815419	19.462323
55.073938	2074.339035	19.467341
55.226025	2079.046760	19.472359
55.033584	2091.124326	19.477376
55.238995	2082.431795	19.482394
55.411170	2084.887581	19.487411
55.430527	2092.197141	19.492429
55.483846	2087.259460	19.497447
55.193274	2083.822301	19.502464
55.601782	2074.969962	19.507482
55.571828	2092.050008	19.512499
55.945517	2104.095498	19.517517
56.208133	2107.985685	19.522535
55.801241	2110.465400	19.527552
56.319668	2112.748771	19.532570
55.977038	2096.284446	19.537587
55.607942	2086.836428	19.542605
56.273049	2087.439146	19.547623
55.939986	2104.267874	19.552640
56.242150	2108.278388	19.557658
56.245761	2106.360323	19.562675
56.394728	2102.318992	19.567693
56.816487	2099.127673	19.572711
56.299415	2111.698284	19.577728
56.837091	2108.101495	19.582746
56.626054	2109.138905	19.587763
56.396074	2098.442462	19.592781
56.751492	2096.513909	19.597799
56.696353	2095.384684	19.602816
56.952079	2104.815627	19.607834
56.691259	2101.633280	19.612851
56.852025	2095.644935	19.617869
57.303770	2089.910647	19.622887
56.981090	2100.805574	19.627904
56.833456	2097.680685	19.632922
57.004595	2096.807181	19.637939
56.690185	2098.848981	19.642957
57.168408	2089.755842	19.647975
57.029562	2094.145802	19.652992
56.891367	2084.071048	19.658010
56.846945	2087.535125	19.663027
56.962359	2096.346617	19.668045
57.050721	2110.610851	19.673063
57.216007	2122.282162	19.678080
57.223571	2124.178229	19.683098
57.767277	2109.000115	19.688115
57.456747	2123.541922	19.693133
57.576413	2112.431824	19.698151
57.550236	2121.338277	19.703168
57.709465	2114.004384	19.708186
57.952665	2124.035114	19.713203
57.873834	2140.422983	19.718221
58.247503	2128.002085	19.723239
57.651333	2139.099543	19.728256
58.313574	2139.159215	19.733274
58.439406	2141.989721	19.738291
58.234283	2148.768009	19.743309
58.524244	2138.190756	19.748327
58.365578	2148.100756	19.753344
58.554464	2148.525374	19.758362
58.513858	2142.532159	19.763379
58.573782	2150.871166	19.768397
58.571738	2141.591097	19.773415
58.475162	2144.427186	19.778432
58.424941	2139.523305	19.783450
58.727491	2147.859009	19.788467
58.681297	2138.077873	19.793485
58.810240	2131.294668	19.798503
58.854559	2137.544720	19.803520
58.673554	2140.864630	19.808538
58.811863	2143.172450	19.813555
58.733349	2139.473357	19.818573
58.902917	2136.083141	19.823591
58.787990	2145.891778	19.828608
59.158078	2159.731224	19.833626
59.428815	2172.158937	19.838643
59.009226	2176.705387	19.843661
59.366334	2163.649206	19.848679
59.402466	2171.275471	19.853696
59.559762	2166.874913	19.858714
59.339068	2175.185539	19.863731
59.463978	2176.964578	19.868749
59.825446	2170.782951	19.873767
59.649913	2175.612962	19.878784
59.381856	2176.035735	19.883802
59.675012	2167.974132	19.888819
59.438532	2180.595223	19.893837
59.479103	2175.370095	19.898855
59.685900	2186.645494	19.903872
60.149260	2185.384015	19.908890
60.300176	2180.846037	19.913907
59.956443	2186.868549	19.918925
59.955506	2189.391289	19.923943
60.079353	2186.654900	19.928960
60.174069	2185.168270	19.933978
60.194616	2177.196546	19.938995
60.206853	2183.041154	19.944013
60.367814	2197.595145	19.949031
60.745319	2207.557320	19.954048
60.654976	2208.300193	19.959066
60.759436	2216.557412	19.964083
60.635448	2218.036361	19.969101
60.920841	2209.486737	19.974119
61.082484	2211.981192	19.979136
60.897697	2218.574575	19.984154
61.431800	2224.096070	19.989171
61.010297	2209.476867	19.994189
61.095230	2216.686364	19.999207
61.383538	2207.398488	20.004224
61.099109	2204.437758	20.009242
61.282399	2201.091745	20.014259
61.201673	2211.769620	20.019277
61.441923	2214.026584	20.024295
61.338000	2203.483788	20.029312
61.475678	2207.978338	20.034330
61.659861	2213.083704	20.039347
61.660937	2208.879517	20.044365
61.471054	2208.489897	20.049383
61.499161	2212.346724	20.054400
61.797285	2212.694931	20.059418
61.387816	2206.799059	20.064435
61.612534	2224.011685	20.069453
61.790803	2228.275599	20.074471
61.966253	2236.809387	20.079488
61.771221	2231.965538	20.084506
61.960613	2237.757531	20.089523
62.306845	2239.966922	20.094541
61.935213	2229.432194	20.099559
61.975001	2225.394084	20.104576
62.052597	2238.819334	20.109594
62.178649	2247.451460	20.114611
62.364386	2253.880367	20.119629
62.670884	2269.727127	20.124647
62.872878	2251.526354	20.129664
62.656311	2270.730184	20.134682
63.145980	2256.581488	20.139699
63.031186	2260.057616	20.144717
62.872381	2260.367006	20.149735
63.165387	2254.994617	20.154752
62.975255	2241.498651	20.159770
62.944215	2249.193089	20.164787
62.810737	2261.369936	20.169805
63.060096	2254.731860	20.174823
63.216872	2252.350449	20.179840
63.054502	2266.639093	20.184858
63.164109	2256.073216	20.189875
63.180870	2252.612170	20.194893
63.136488	2246.210505	20.199911
63.228846	2256.878899	20.204928
63.333848	2277.798846	20.209946
63.480047	2275.512719	20.214963
63.588206	2279.395338	20.219981
63.482715	2282.254112	20.224999
63.687721	2279.096538	20.230016
63.686780	2282.851045	20.235034
63.768393	2271.810606	20.240051
63.692417	2285.093641	20.245069
63.694895	2299.597500	20.250087
63.728633	2309.627943	20.255104
63.923755	2309.192649	20.260122
64.289675	2312.215359	20.265139
64.290906	2315.130269	20.270157
64.450204	2311.379833	20.275175
64.770910	2305.708048	20.280192
64.418796	2317.057743	20.285210
64.732682	2298.435560	20.290227
64.577167	2309.688610	20.295245
64.449939	2305.041574	20.300263
64.608888	2299.369633	20.305280
64.719840	2301.473404	20.310298
65.032312	2315.631307	20.315315
65.263561	2327.860159	20.320333
65.334588	2310.802621	20.325351
65.268284	2302.077785	20.330368
65.231053	2306.896794	20.335386
65.217966	2298.417531	20.340403
65.260850	2297.042982	20.345421
65.466352	2285.785349	20.350439
65.537851	2296.198320	20.355456
65.423961	2295.850064	20.360474
65.545425	2288.154784	20.365491
65.439774	2302.281825	20.370509
65.523735	2299.939550	20.375527
66.068644	2289.117023	20.380544
65.632701	2296.353000	20.385562
65.893784	2292.792414	20.390579
66.004241	2296.872098	20.395597
65.993072	2306.318995	20.400615
65.755702	2300.667000	20.405632
65.725746	2307.942846	20.410650
65.906724	2314.237250	20.415667
65.600146	2321.537556	20.420685
65.771114	2320.940149	20.425703
66.176888	2318.730602	20.430720
65.915835	2330.578621	20.435738
66.344022	2333.625228	20.440755
66.595497	2347.073973	20.445773
66.598009	2359.076621	20.450791
66.852630	2344.476872	20.455808
66.657470	2352.070115	20.460826
66.963127	2347.149522	20.465843
67.003847	2344.151851	20.470861
67.131030	2352.301697	20.475879
67.401611	2342.931614	20.480896
67.062535	2329.615846	20.485914
67.421617	2318.502804	20.490931
67.203840	2316.245617	20.495949
67.199617	2310.266980	20.500967
67.252353	2313.572461	20.505984
66.970996	2336.574783	20.511002
67.129960	2330.883950	20.516019
67.096121	2335.466460	20.521037
67.105771	2339.103668	20.526055
67.346631	2350.257351	20.531072
67.205455	2349.583089	20.536090
67.574053	2353.463520	20.541107
67.453422	2375.578985	20.546125
66.963686	2365.051982	20.551143
67.586266	2368.902923	20.556160
67.571523	2377.638598	20.561178
67.632069	2387.492562	20.566195
67.747051	2389.620872	20.571213
67.874775	2404.305435	20.576231
68.516759	2395.921430	20.581248
68.395298	2387.432656	20.586266
68.158762	2395.214216	20.591283
68.778798	2390.675293	20.596301
68.684669	2394.693245	20.601319
69.102020	2383.534679	20.606336
68.687104	2399.336963	20.611354
68.879634	2380.782011	20.616371
69.004688	2378.681724	20.621389
68.705174	2396.100078	20.626407
69.124652	2373.141152	20.631424
69.094408	2384.528446	20.636442
68.978099	2379.262193	20.641459
69.091267	2378.014076	20.646477
69.365551	2372.842844	20.651495
69.446070	2374.495272	20.656512
68.969140	2378.866085	20.661530
69.073921	2382.971868	20.666547
68.725578	2372.659851	20.671565
69.132066	2392.666663	20.676583
69.214469	2397.590900	20.681600
69.302414	2406.373926	20.686618
69.466708	2412.218759	20.691635
69.485673	2410.322589	20.696653
69.110911	2414.302713	20.701671
69.508906	2416.542419	20.706688
69.543602	2443.505200	20.711706
69.800856	2435.953365	20.716723
69.854680	2444.965242	20.721741
69.838816	2444.369311	20.726759
70.139210	2435.180044	20.731776
70.100078	2442.877447	20.736794
70.666094	2454.023401	20.741811
70.681526	2455.029435	20.746829
70.546232	2449.114120	20.751847
70.572324	2451.124473	20.756864
70.671740	2460.910149	20.761882
70.933691	2454.823718	20.766899
71.144421	2456.491572	20.771917
70.762373	2443.317055	20.776935
71.100882	2440.105907	20.781952
71.356193	2448.982612	20.786970
70.982579	2436.510734	20.791987
71.022288	2432.595283	20.797005
71.250904	2439.026873	20.802023
71.319800	2441.134225	20.807040
71.338851	2450.135919	20.812058
71.292034	2441.290693	20.817075
71.848247	2451.367692	20.822093
71.452898	2452.215853	20.827111
71.385431	2448.923147	20.832128
71.594522	2451.849769	20.837146
71.445548	2448.277459	20.842163
71.707593	2443.276480	20.847181
71.752436	2452.416431	20.852199
71.997369	2440.254917	20.857216
71.706073	2451.339381	20.862234
71.589210	2457.936983	20.867251
72.302759	2453.894397	20.872269
71.953803	2476.360269	20.877287
72.271288	2476.822595	20.882304
72.314752	2472.120753	20.887322
72.025288	2476.751940	20.892339
72.438117	2476.136406	20.897357
72.454335	2480.854133	20.902375
72.430856	2463.608553	20.907392
72.464277	2475.348373	20.912410
72.547276	2489.178076	20.917427
72.755245	2496.258757	20.922445
72.733165	2505.081414	20.927463
72.887557	2500.200626	20.932480
72.943701	2500.797446	20.937498
72.722387	2498.983633	20.942515
73.058759	2496.567249	20.947533
72.819020	2501.837860	20.952551
73.110338	2488.025765	20.957568
73.182134	2505.349636	20.962586
73.205229	2526.607857	20.967603
73.948278	2524.450679	20.972621
73.769635	2529.062635	20.977639
73.802063	2525.150681	20.982656
73.894176	2520.269592	20.987674
74.061658	2527.421245	20.992691
74.311745	2528.291539	20.997709
74.090183	2507.242178	21.002727
74.289008	2488.964530	21.007744
74.093349	2493.620877	21.012762
73.723591	2493.676030	21.017779
74.402409	2500.605325	21.022797
74.209449	2514.652107	21.027815
74.353732	2512.836619	21.032832
74.323866	2524.876816	21.037850
74.215113	2517.958295	21.042867
74.411511	2520.515693	21.047885
74.473475	2518.422301	21.052903
74.614100	2523.374264	21.057920
74.399034	2515.767145	21.062938
74.370225	2531.107629	21.067955
74.918889	2531.807602	21.072973
74.376338	2539.982560	21.077991
74.801230	2538.259181	21.083008
74.718058	2534.249247	21.088026
74.838714	2552.301613	21.093043
75.016330	2558.807462	21.098061
74.998212	2570.203980	21.103079
75.208069	2559.723363	21.108096
75.415404	2559.193299	21.113114
75.089435	2559.074714	21.118131
75.695433	2579.531349	21.123149
75.778376	2592.222199	21.128167
75.788466	2591.517508	21.133184
75.737009	2594.602911	21.138202
75.677317	2595.458115	21.143219
75.968707	2588.902068	21.148237
75.725194	2593.753283	21.153255
75.928133	2583.952566	21.158272
76.566638	2609.086535	21.163290
76.290701	2618.944765	21.168307
76.851837	2616.692306	21.173325
76.776874	2614.947953	21.178343
76.633143	2607.098942	21.183360
76.978972	2590.369302	21.188378
76.808539	2588.662988	21.193395
77.028711	2583.392553	21.198413
76.570673	2576.255193	21.203431
76.538051	2580.214619	21.208448
76.597664	2593.939603	21.213466
76.614309	2602.913458	21.218483
77.335171	2603.763739	21.223501
77.314009	2607.516835	21.228519
77.319014	2602.261830	21.233536
77.409483	2604.777930	21.238554
77.330161	2598.607429	21.243571
77.537041	2601.222164	21.248589
77.497612	2595.886937	21.253607
77.316769	2609.952329	21.258624
77.640260	2597.657024	21.263642
77.620724	2611.201937	21.268659
78.014865	2621.771343	21.273677
78.136244	2620.348849	21.278695
77.899929	2636.349439	21.283712
77.969903	2638.053920	21.288730
78.005637	2627.908575	21.293747
78.340672	2632.440215	21.298765
78.001761	2629.860135	21.303783
78.083547	2627.149250	21.308800
78.373913	2629.503691	21.313818
78.263349	2636.355219	21.318835
78.387212	2643.424216	21.323853
78.331450	2650.580069	21.328871
78.768606	2660.932627	21.333888
78.830804	2653.586410	21.338906
78.442742	2658.067409	21.343923
78.642104	2661.045966	21.348941
78.895952	2675.839688	21.353959
78.877517	2675.460467	21.358976
79.326964	2676.999033	21.363994
79.059141	2684.358623	21.369011
79.587510	2669.267330	21.374029
79.637412	2675.648869	21.379047
79.641520	2674.204171	21.384064
79.772535	2671.665553	21.389082
79.628535	2677.700459	21.394099
80.009444	2670.334868	21.399117
80.278636	2670.462741	21.404135
80.134341	2669.589956	21.409152
80.428619	2666.024774	21.414170
80.252283	2678.158462	21.419187
80.467049	2660.252470	21.424205
80.285498	2670.482678	21.429223
80.201140	2662.134916	21.434240
80.395988	2667.054684	21.439258
80.131530	2669.313554	21.444275
80.692267	2668.915906	21.449293
80.632679	2662.257698	21.454311
80.831787	2658.271931	21.459328
81.054488	2665.112013	21.464346
80.613061	2656.071590	21.469363
80.864848	2681.346017	21.474381
81.162784	2674.692139	21.479399
80.885128	2683.464420	21.484416
80.953812	2689.577106	21.489434
81.297653	2694.259959	21.494451
81.384010	2685.852708	21.499469
81.111447	2683.230574	21.504487
81.061764	2692.203263	21.509504
81.364963	2687.379699	21.514522
81.265929	2700.043818	21.519539
81.487555	2709.740166	21.524557
81.630013	2714.377270	21.529575
81.492462	2727.797167	21.534592
81.990067	2717.660692	21.539610
82.124486	2727.126333	21.544627
81.838749	2723.627680	21.549645
81.597586	2716.323518	21.554663
82.082649	2744.801568	21.559680
82.081911	2742.120341	21.564698
82.191440	2745.176955	21.569715
82.605496	2755.007042	21.574733
82.501397	2745.929284	21.579751
82.791978	2743.070238	21.584768
82.781722	2742.555205	21.589786
82.612279	2751.592652	21.594803
83.122938	2744.970891	21.599821
83.251797	2743.253011	21.604839
82.697909	2746.493298	21.609856
82.851625	2746.332034	21.614874
83.027635	2772.446976	21.619891
83.553257	2765.217150	21.624909
83.276464	2782.478169	21.629927
82.935483	2779.336770	21.634944
83.698950	2769.614866	21.639962
83.628357	2769.822100	21.644979
83.508547	2777.194314	21.649997
83.519165	2769.562868	21.655015
83.644135	2788.445472	21.660032
83.985762	2785.462650	21.665050
83.786986	2796.045722	21.670067
84.123937	2800.148422	21.675085
84.209456	2785.658580	21.680103
84.461500	2784.817757	21.685120
84.544774	2792.115116	21.690138
84.304225	2794.903498	21.695155
84.665853	2787.356076	21.700173
84.755814	2783.296438	21.705191
84.590616	2794.477465	21.710208
84.924278	2787.634565	21.715226
84.881131	2785.476093	21.720243
84.856227	2794.897967	21.725261
85.108612	2809.474175	21.730279
85.410866	2811.000834	21.735296
85.321159	2805.851317	21.740314
85.111919	2812.676189	21.745331
85.337810	2803.662971	21.750349
85.423259	2797.860188	21.755367
85.232488	2812.244351	21.760384
85.418729	2810.607770	21.765402
85.352581	2800.402254	21.770419
85.571939	2804.966556	21.775437
85.833214	2810.979360	21.780455
85.937987	2811.440225	21.785472
86.023895	2793.913303	21.790490
85.821017	2822.962157	21.795507
85.859522	2835.584794	21.800525
86.208896	2830.679094	21.805543
85.780974	2841.593713	21.810560
86.187687	2834.378097	21.815578
86.273706	2832.615124	21.820595
86.204707	2841.437601	21.825613
86.318175	2852.012607	21.830631
86.681739	2853.797721	21.835648
86.678247	2850.386959	21.840666
86.563883	2862.984444	21.845683
86.714501	2860.168935	21.850701
87.053458	2863.696336	21.855719
86.839649	2890.921394	21.860736
87.241728	2885.829501	21.865754
87.409349	2891.571741	21.870771
87.288176	2891.197099	21.875789
87.743131	2884.434708	21.880807
87.810766	2884.789016	21.885824
87.681013	2890.059530	21.890842
87.416047	2895.516793	21.895859
87.740469	2886.751319	21.900877
87.900294	2882.243955	21.905895
87.641560	2892.966447	21.910912
87.962699	2901.430984	21.915930
87.961683	2904.074209	21.920947
87.913506	2904.633409	21.925965
88.007815	2905.019647	21.930983
88.200771	2915.275252	21.936000
88.577273	2923.203957	21.941018
88.580534	2936.524503	21.946035
88.505857	2939.240050	21.951053
89.032799	2933.720772	21.956071
88.826637	2942.001197	21.961088
88.947167	2927.172116	21.966106
89.274548	2935.990432	21.971123
89.159899	2933.083492	21.976141
89.213854	2930.877263	21.981159
89.377244	2925.875336	21.986176
89.494538	2923.305040	21.991194
89.437489	2926.274202	21.996211
89.648535	2915.252753	22.001229
89.879221	2922.274959	22.006247
89.608955	2935.756328	22.011264
90.095768	2930.986782	22.016282
90.265106	2941.488443	22.021299
90.204368	2918.178913	22.026317
89.934786	2911.012118	22.031335
89.844829	2933.200621	22.036352
90.035859	2939.024886	22.041370
90.186569	2945.881302	22.046387
89.851648	2947.014036	22.051405
90.178125	2947.399433	22.056423
90.162351	2950.339993	22.061440
90.767060	2965.504391	22.066458
90.757261	2975.325923	22.071475
91.163811	2975.733948	22.076493
91.215027	2978.906889	22.081511
91.081405	2975.327280	22.086528
91.247107	2974.179286	22.091546
91.402503	2972.713578	22.096563
90.718986	2988.456285	22.101581
91.228656	2964.996720	22.106599
91.413502	2965.485724	22.111616
91.291466	2974.993211	22.116634
91.584301	2977.328438	22.121651
91.968031	2980.449138	22.126669
91.863904	2994.689089	22.131687
91.437716	2988.241008	22.136704
91.924184	2987.683722	22.141722
92.278215	2999.032239	22.146739
91.999116	2996.473229	22.151757
92.085618	2987.855761	22.156775
92.034320	2995.593152	22.161792
92.290183	3017.178376	22.166810
92.274900	3014.472674	22.171827
92.553238	3021.617905	22.176845
92.729708	3022.543235	22.181863
92.850570	3030.505688	22.186880
93.060264	3009.282207	22.191898
93.044918	3014.026379	22.196915
92.967006	3026.541104	22.201933
93.400676	3005.480920	22.206951
93.379342	3018.070782	22.211968
93.351416	3014.909296	22.216986
93.688671	3027.169031	22.222003
93.531657	3024.708537	22.227021
93.982725	3037.349722	22.232039
93.785402	3040.806943	22.237056
94.039125	3032.545855	22.242074
94.170249	3024.961918	22.247091
94.098851	3039.863728	22.252109
93.998057	3036.793305	22.257127
94.112101	3041.604164	22.262144
93.960959	3038.825731	22.267162
94.132194	3031.752977	22.272179
93.838255	3044.316327	22.277197
94.238001	3055.049557	22.282215
94.606433	3061.748597	22.287232
94.412619	3069.693606	22.292250
94.614004	3064.740635	22.297267
94.429168	3076.241222	22.302285
95.294050	3074.755179	22.307303
95.073699	3089.811370	22.312320
94.878713	3093.400379	22.317338
95.077136	3100.291736	22.322355
95.506017	3098.755658	22.327373
95.462913	3092.848975	22.332391
95.512769	3096.859102	22.337408
95.539025	3101.080657	22.342426
95.754414	3084.718934	22.347443
96.065996	3096.663462	22.352461
95.795655	3093.078096	22.357479
95.839967	3089.554250	22.362496
96.034657	3093.523974	22.367514
96.448121	3107.996134	22.372531
96.248417	3128.536411	22.377549
96.508473	3118.042671	22.382567
96.182763	3118.677601	22.387584
96.211059	3124.710385	22.392602
96.441582	3116.062794	22.397619
96.093225	3117.916638	22.402637
96.694389	3129.914125	22.407655
96.628376	3134.203892	22.412672
96.777117	3141.605044	22.417690
96.767783	3148.269975	22.422707
96.795763	3148.653425	22.427725
97.206095	3164.199069	22.432743
97.104908	3171.526822	22.437760
97.510073	3186.320532	22.442778
97.695160	3169.297291	22.447795
97.943456	3176.625949	22.452813
98.388795	3155.071274	22.457831
98.639091	3161.822238	22.462848
98.511060	3162.017398	22.467866
98.898554	3159.466114	22.472883
98.376891	3153.004079	22.477901
98.565845	3150.960354	22.482919
98.438207	3145.657084	22.487936
98.736484	3150.804371	22.492954
98.788411	3148.000613	22.497971
98.812624	3147.964617	22.502989
98.874658	3147.006982	22.508007
98.599809	3151.470074	22.513024
98.671190	3143.705245	22.518042
99.396871	3138.664706	22.523059
98.994940	3148.134348	22.528077
99.220501	3148.237722	22.533095
99.246316	3146.998752	22.538112
98.943607	3160.576747	22.543130
99.406005	3167.112183	22.548147
99.379433	3179.057216	22.553165
99.438076	3174.659504	22.558183
99.571294	3174.941219	22.563200
99.604890	3191.332004	22.568218
99.723824	3192.419123	22.573235
99.458553	3209.332699	22.578253
99.897809	3204.355907	22.583271
100.116553	3202.532394	22.588288
99.941518	3213.882071	22.593306
100.367850	3223.585449	22.598323
100.389502	3226.203880	22.603341
100.702983	3235.288109	22.608359
100.829068	3237.799428	22.613376
100.558474	3240.711460	22.618394
100.893063	3228.847281	22.623411
100.706208	3232.361873	22.628429
101.121390	3250.383082	22.633447
101.111792	3266.028840	22.638464
100.891934	3257.033725	22.643482
101.580499	3262.894411	22.648499
101.384713	3271.358219	22.653517
101.376056	3250.029980	22.658535
101.783129	3269.310296	22.663552
101.922922	3274.342883	22.668570
102.013716	3267.811446	22.673587
101.764325	3286.399634	22.678605
102.438809	3276.829250	22.683623
102.329541	3275.555961	22.688640
102.025034	3274.686661	22.693658
102.242245	3271.515919	22.698675
102.050308	3302.340148	22.703693
102.188756	3294.702201	22.708711
102.470286	3297.042431	22.713728
102.551943	3298.228323	22.718746
102.837420	3306.848242	22.723763
102.774334	3326.311375	22.728781
103.252589	3327.228718	22.733799
103.341252	3336.186034	22.738816
103.004402	3331.607493	22.743834
103.592702	3327.596454	22.748851
103.697083	3327.448560	22.753869
103.732320	3324.195127	22.758887
104.041218	3323.074615	22.763904
104.011539	3322.565018	22.768922
104.054090	3343.777277	22.773939
104.440916	3349.617682	22.778957
104.492759	3350.621904	22.783975
104.576637	3342.313786	22.788992
104.689954	3333.530582	22.794010
104.773023	3322.772300	22.799027
104.955540	3328.045090	22.804045
104.835362	3323.686076	22.809063
104.847331	3326.267524	22.814080
104.862266	3329.257539	22.819098
105.147352	3334.800303	22.824115
105.156254	3335.900260	22.829133
105.117839	3338.819337	22.834151
105.549905	3334.959069	22.839168
105.630579	3349.893580	22.844186
105.640211	3331.499528	22.849203
105.702028	3335.779195	22.854221
105.736305	3327.851064	22.859239
105.924627	3336.587968	22.864256
105.366974	3329.451957	22.869274
105.827828	3326.102333	22.874291
105.647750	3335.274772	22.879309
105.785480	3352.020414	22.884327
105.888841	3353.419955	22.889344
105.997036	3362.206623	22.894362
106.449115	3364.802062	22.899379
106.550483	3376.577397	22.904397
106.271654	3383.368005	22.909415
106.599455	3379.358377	22.914432
106.482525	3388.464143	22.919450
106.846549	3388.410928	22.924467
107.037871	3414.670104	22.929485
106.964892	3420.926827	22.934503
107.083624	3410.070759	22.939520
106.844252	3429.400098	22.944538
107.171379	3421.510957	22.949555
107.548497	3442.074536	22.954573
107.672685	3441.341383	22.959591
107.968964	3443.418127	22.964608
107.976692	3441.393037	22.969626
108.268666	3438.962346	22.974643
108.367195	3428.073302	22.979661
108.329292	3435.118924	22.984679
108.610598	3434.142823	22.989696
108.340584	3431.247971	22.994714
108.651783	3446.272466	22.999731
109.076032	3451.820614	23.004749
108.472618	3463.738300	23.009767
108.879773	3465.765115	23.014784
109.074365	3466.235278	23.019802
109.300119	3451.363715	23.024819
109.355745	3456.445186	23.029837
109.208159	3466.640640	23.034855
109.467925	3454.172286	23.039872
109.370221	3484.402917	23.044890
109.655961	3474.261168	23.049907
109.774283	3481.192225	23.054925
109.666654	3484.781557	23.059943
110.098848	3481.975306	23.064960
109.928049	3488.111571	23.069978
110.441735	3483.194401	23.074995
110.785940	3503.381017	23.080013
110.397797	3490.680064	23.085031
110.954499	3497.818899	23.090048
110.733895	3513.219318	23.095066
110.715273	3510.664302	23.100083
111.147319	3505.635857	23.105101
111.258305	3513.877827	23.110119
111.148835	3520.255259	23.115136
111.102823	3510.165602	23.120154
111.224413	3512.147501	23.125171
111.279129	3511.254726	23.130189
110.814171	3509.513458	23.135207
111.362693	3511.887451	23.140224
111.141026	3530.123837	23.145242
111.431302	3542.533879	23.150259
111.709859	3528.571024	23.155277
111.397537	3549.316279	23.160295
111.772937	3550.435684	23.165312
111.937604	3561.929688	23.170330
111.925437	3570.433610	23.175347
112.266552	3563.435772	23.180365
112.126739	3596.171676	23.185383
112.749191	3594.416679	23.190400
112.895295	3594.809623	23.195418
112.663089	3603.265271	23.200435
113.116365	3588.145684	23.205453
112.750372	3597.039575	23.210471
112.943341	3613.462056	23.215488
113.100957	3620.930474	23.220506
113.317576	3615.004976	23.225523
113.355035	3630.454041	23.230541
113.488719	3631.276107	23.235559
113.730627	3639.748993	23.240576
114.202488	3652.867246	23.245594
113.760601	3654.157107	23.250611
114.554283	3646.735437	23.255629
114.294858	3644.941711	23.260647
114.396329	3643.084929	23.265664
114.387393	3649.146678	23.270682
114.443888	3648.012902	23.275699
114.627501	3643.063359	23.280717
114.899636	3656.003434	23.285735
115.046203	3661.828001	23.290752
114.916330	3673.369847	23.295770
114.898919	3656.720518	23.300787
115.388424	3656.596951	23.305805
115.473284	3657.843719	23.310823
115.386548	3654.289504	23.315840
115.415427	3679.061580	23.320858
115.890378	3670.344008	23.325875
116.059004	3685.654221	23.330893
116.143174	3684.270599	23.335911
116.356625	3670.893807	23.340928
116.541301	3680.275751	23.345946
116.568264	3673.624518	23.350963
116.765186	3679.163381	23.355981
116.798613	3668.848555	23.360999
117.055850	3671.269025	23.366016
116.549138	3673.915940	23.371034
116.740561	3673.075299	23.376051
116.979233	3670.523277	23.381069
116.853313	3683.428523	23.386087
116.967000	3675.327067	23.391104
117.352312	3685.971819	23.396122
117.133631	3697.217126	23.401139
117.568415	3702.781784	23.406157
117.008776	3699.804055	23.411175
117.544774	3697.900787	23.416192
117.735965	3719.480059	23.421210
117.875882	3731.707355	23.426227
118.434933	3729.207284	23.431245
118.081033	3735.691437	23.436263
118.032550	3734.245581	23.441280
118.066185	3722.389664	23.446298
117.980332	3744.464680	23.451315
118.299295	3748.987440	23.456333
118.408440	3764.931811	23.461351
118.510323	3753.875223	23.466368
118.723011	3777.212433	23.471386
118.649916	3787.312060	23.476403
119.017554	3789.191043	23.481421
118.912916	3791.916244	23.486439
119.218892	3807.536643	23.491456
119.587736	3812.495134	23.496474
119.644992	3812.662327	23.501491
119.655254	3810.476307	23.506509
119.691459	3808.212992	23.511527
120.011019	3824.097128	23.516544
120.163201	3838.585723	23.521562
120.201043	3848.553639	23.526579
120.452458	3829.155197	23.531597
120.213707	3847.508764	23.536615
120.411884	3833.991090	23.541632
121.052932	3844.577085	23.546650
121.070125	3857.634297	23.551667
121.175813	3853.074699	23.556685
121.175402	3857.253526	23.561703
121.603587	3848.318329	23.566720
121.809205	3850.501628	23.571738
121.862978	3843.688714	23.576755
121.975466	3847.217075	23.581773
121.860883	3851.520304	23.586791
121.659520	3843.870181	23.591808
122.181903	3840.556259	23.596826
121.892455	3849.901427	23.601843
122.088515	3842.047123	23.606861
122.013373	3860.149637	23.611879
122.400074	3873.616780	23.616896
122.282467	3875.146006	23.621914
122.382900	3888.358314	23.626931
122.806006	3883.446805	23.631949
122.882299	3895.230489	23.636967
122.849149	3903.651420	23.641984
123.372447	3897.732757	23.647002
123.417378	3911.673716	23.652019
123.490936	3899.403808	23.657037
123.172649	3898.496545	23.662055
123.577409	3901.770639	23.667072
123.711189	3917.176329	23.672090
123.660377	3921.706976	23.677107
124.141369	3935.757778	23.682125
123.873128	3928.902563	23.687143
124.134168	3940.292606	23.692160
124.343899	3926.441827	23.697178
124.371914	3931.685195	23.702195
124.612030	3945.355921	23.707213
124.687636	3955.730878	23.712231
124.708935	3953.986746	23.717248
125.264683	3958.986282	23.722266
125.054563	3948.658964	23.727283
125.125685	3944.984321	23.732301
125.232768	3946.899368	23.737319
125.340234	3956.814563	23.742336
125.553223	3966.227576	23.747354
125.541898	3983.264383	23.752371
125.757911	3980.739522	23.757389
125.597160	3977.751618	23.762407
125.820854	3980.754890	23.767424
125.969000	3990.334801	23.772442
125.879023	4014.974574	23.777459
126.604197	4009.704129	23.782477
126.615310	4005.003808	23.787495
126.233798	4007.929742	23.792512
126.586646	4013.859220	23.797530
126.839517	4040.087679	23.802547
127.009503	4038.648648	23.807565
126.976193	4041.179230	23.812583
127.263990	4029.203086	23.817600
127.614807	4044.346171	23.822618
127.747561	4056.408110	23.827635
128.195747	4045.400707	23.832653
128.195424	4049.445844	23.837671
128.106648	4055.098847	23.842688
128.351946	4048.668290	23.847706
128.490330	4052.202799	23.852723
128.063225	4039.603549	23.857741
128.082774	4051.545085	23.862759
128.239594	4038.179350	23.867776
128.556041	4056.359687	23.872794
128.608583	4066.128744	23.877811
128.823707	4066.185809	23.882829
128.556635	4059.995067	23.887847
128.892789	4082.645995	23.892864
129.312099	4085.972091	23.897882
129.370464	4095.499522	23.902899
129.826229	4088.955936	23.907917
129.649748	4099.983997	23.912935
129.862321	4101.456662	23.917952
130.081290	4123.890344	23.922970
130.024295	4130.430376	23.927987
130.266234	4132.773125	23.933005
130.322854	4132.686334	23.938023
129.993556	4138.627878	23.943040
130.442671	4132.353584	23.948058
130.445403	4157.516886	23.953075
130.805285	4150.354515	23.958093
130.511081	4166.876542	23.963111
130.796461	4159.800779	23.968128
131.136468	4163.136392	23.973146
131.250063	4180.938595	23.978163
131.290976	4183.808217	23.983181
131.724914	4177.240539	23.988199
131.447269	4187.060754	23.993216
131.719857	4171.170138	23.998234
132.040406	4181.923127	24.003251
132.227526	4193.767258	24.008269
132.353614	4202.450100	24.013287
132.591040	4207.960679	24.018304
133.039359	4205.358618	24.023322
132.733557	4206.341263	24.028339
133.106032	4202.178760	24.033357
133.303479	4209.412997	24.038375
133.227439	4200.668123	24.043392
133.150688	4195.452329	24.048410
133.013041	4201.582816	24.053427
133.218022	4194.948587	24.058445
133.220163	4221.007313	24.063463
133.448571	4221.791497	24.068480
133.958774	4216.161142	24.073498
133.534281	4231.455585	24.078515
133.565640	4243.895711	24.083533
133.636429	4250.542074	24.088551
133.917555	4252.374343	24.093568
134.218890	4266.499740	24.098586
134.102163	4278.939909	24.103603
134.518388	4285.737312	24.108621
134.621476	4292.490251	24.113639
134.891640	4304.803457	24.118656
135.253969	4307.440918	24.123674
135.279001	4320.886692	24.128691
135.338486	4310.329687	24.133709
135.654279	4302.555167	24.138727
135.643093	4312.023029	24.143744
136.411447	4321.109355	24.148762
136.486901	4329.273278	24.153779
136.608366	4325.349006	24.158797
136.609486	4318.625295	24.163815
136.492659	4316.500371	24.168832
136.781231	4332.807723	24.173850
136.615584	4338.442412	24.178867
136.555468	4339.898011	24.183885
136.693523	4326.778086	24.188903
136.691574	4330.834574	24.193920
136.778427	4336.440012	24.198938
137.000956	4354.723804	24.203955
137.164814	4354.005523	24.208973
137.599223	4361.468731	24.213991
137.439978	4374.568698	24.219008
137.960875	4378.507214	24.224026
137.862947	4378.397864	24.229043
137.813201	4381.306368	24.234061
138.056302	4392.946640	24.239079
137.759292	4385.494779	24.244096
138.264136	4399.045051	24.249114
138.608097	4418.491141	24.254131
138.552513	4414.304794	24.259149
138.941836	4409.160927	24.264167
138.894581	4410.746643	24.269184
139.133365	4421.574994	24.274202
139.419213	4438.339168	24.279219
139.042514	4441.271497	24.284237
139.683603	4444.580408	24.289255
139.596538	4442.724482	24.294272
139.736937	4443.223776	24.299290
139.986162	4450.493930	24.304307
140.257654	4458.359984	24.309325
140.246554	4459.116291	24.314343
140.127328	4461.847087	24.319360
140.812965	4447.938027	24.324378
140.889543	4456.854689	24.329395
140.664328	4454.644760	24.334413
140.847398	4465.287719	24.339431
140.716340	4481.040675	24.344448
141.289405	4478.299888	24.349466
141.297800	4477.718885	24.354483
141.407541	4478.078321	24.359501
141.610514	4500.256313	24.364519
141.587485	4504.370490	24.369536
141.835100	4494.468551	24.374554
142.289492	4497.427280	24.379571
142.275904	4505.630673	24.384589
142.255163	4506.278385	24.389607
142.324414	4520.168058	24.394624
142.519331	4522.674131	24.399642
142.927347	4539.498396	24.404659
142.969760	4522.934519	24.409677
143.124576	4528.570889	24.414695
142.961358	4546.453862	24.419712
143.304103	4543.237661	24.424730
143.160020	4552.973100	24.429747
143.631116	4550.247773	24.434765
143.806927	4551.052163	24.439783
143.950455	4559.077918	24.444800
144.065962	4569.097661	24.449818
144.049571	4580.321611	24.454835
144.276769	4586.645821	24.459853
144.433574	4573.331524	24.464871
144.107433	4585.471791	24.469888
144.949634	4599.231996	24.474906
144.971008	4598.604865	24.479923
145.020943	4608.655545	24.484941
145.073848	4603.170339	24.489959
144.988560	4609.652161	24.494976
145.419958	4625.395828	24.499994
145.685803	4636.931973	24.505011
145.804663	4633.288881	24.510029
145.912531	4640.171807	24.515047
145.719511	4638.214749	24.520064
146.071077	4633.907564	24.525082
146.273083	4640.395511	24.530099
146.382635	4658.214672	24.535117
146.729928	4645.669209	24.540135
146.688890	4661.127943	24.545152
146.636221	4653.745546	24.550170
146.610089	4656.430067	24.555187
146.823522	4677.487206	24.560205
147.263348	4678.018219	24.565223
147.087533	4679.419924	24.570240
147.494651	4681.687652	24.575258
147.824868	4695.019812	24.580275
147.885410	4712.298532	24.585293
148.290019	4703.656870	24.590311
148.420396	4713.225142	24.595328
148.677345	4703.913951	24.600346
148.621832	4703.291995	24.605363
148.529267	4715.890738	24.610381
149.018048	4699.888773	24.615399
148.737383	4710.550785	24.620416
149.062581	4726.587623	24.625434
149.139102	4731.920306	24.630451
149.187575	4727.021844	24.635469
149.545591	4719.086183	24.640487
149.786119	4737.111122	24.645504
149.791350	4748.681044	24.650522
150.224207	4761.013535	24.655539
150.273508	4754.860947	24.660557
150.315536	4747.465763	24.665575
150.248561	4758.077215	24.670592
150.469340	4753.298382	24.675610
150.548793	4760.321994	24.680627
150.598212	4778.515914	24.685645
150.767907	4782.468061	24.690663
150.692078	4789.326853	24.695680
150.896961	4795.145721	24.700698
151.008639	4808.524631	24.705715
150.856664	4828.977856	24.710733
151.327841	4824.946555	24.715751
151.589739	4837.576994	24.720768
152.007452	4837.301245	24.725786
152.501561	4856.165422	24.730803
152.925496	4851.372259	24.735821
152.834276	4857.024384	24.740839
152.441323	4852.642323	24.745856
153.069182	4840.534204	24.750874
152.822689	4857.043101	24.755891
152.677009	4860.597925	24.760909
153.070502	4861.463601	24.765927
153.136674	4883.706468	24.770944
153.129829	4882.917831	24.775962
154.116081	4868.581259	24.780979
153.877015	4876.285857	24.785997
153.797222	4871.982088	24.791015
153.951092	4896.239882	24.796032
154.163753	4897.638668	24.801050
154.622656	4886.470808	24.806067
154.484493	4901.933482	24.811085
155.138217	4891.118464	24.816103
154.573037	4893.836269	24.821120
154.780724	4905.226133	24.826138
154.851000	4911.440979	24.831155
154.908121	4924.099424	24.836173
155.174260	4926.635907	24.841191
155.309028	4945.501640	24.846208
155.330190	4952.556666	24.851226
155.996400	4946.129412	24.856243
155.814275	4968.109903	24.861261
156.229459	4975.365658	24.866279
156.424128	4980.731516	24.871296
156.467848	4980.586201	24.876314
156.720528	4981.446016	24.881331
156.797982	4982.919078	24.886349
157.190737	4994.732644	24.891367
156.867218	5002.852779	24.896384
157.187883	5003.714343	24.901402
157.505016	5002.572734	24.906419
157.487762	5022.460347	24.911437
158.026808	5022.321804	24.916455
158.418810	5036.509014	24.921472
158.473366	5033.435426	24.926490
158.678013	5028.593780	24.931507
158.483673	5038.418583	24.936525
158.901317	5034.603453	24.941543
158.687782	5037.948075	24.946560
158.701222	5037.082245	24.951578
158.866728	5040.039161	24.956595
158.713051	5059.380574	24.961613
159.272152	5047.258863	24.966631
159.365309	5058.052689	24.971648
159.472870	5078.907008	24.976666
159.904221	5077.627603	24.981683
159.745078	5083.174999	24.986701
160.091906	5098.367017	24.991719
160.367021	5103.260655	24.996736
160.402655	5115.368060	25.001754
160.633595	5108.709616	25.006771
160.276664	5114.708663	25.011789
160.982571	5137.696411	25.016807
160.916956	5136.429370	25.021824
161.136343	5141.145456	25.026842
161.254370	5143.690646	25.031859
161.335850	5162.368476	25.036877
161.740363	5153.935048	25.041895
161.746851	5172.187436	25.046912
161.971901	5169.550796	25.051930
162.361380	5159.373260	25.056947
162.177802	5193.354047	25.061965
162.604075	5186.291522	25.066983
162.748517	5188.060742	25.072000
162.682139	5189.175988	25.077018
163.116168	5183.854798	25.082035
163.240706	5182.670721	25.087053
163.299590	5196.343979	25.092071
163.683048	5207.556577	25.097088
163.961777	5206.986726	25.102106
164.042566	5207.092754	25.107123
163.755136	5198.524960	25.112141
164.021437	5205.747926	25.117159
164.502277	5200.637974	25.122176
163.994052	5210.202185	25.127194
164.496162	5226.825788	25.132211
164.527477	5231.988850	25.137229
164.862850	5236.348972	25.142247
165.182588	5237.419965	25.147264
165.200050	5250.082653	25.152282
165.287393	5254.976387	25.157299
165.259974	5248.567554	25.162317
165.352483	5252.992366	25.167335
165.536129	5277.533981	25.172352
165.742863	5271.998824	25.177370
165.826007	5290.613615	25.182387
166.108620	5307.466627	25.187405
166.359117	5303.078600	25.192423
166.683363	5324.305452	25.197440
166.710901	5335.192550	25.202458
167.094909	5344.362049	25.207475
166.934005	5347.657438	25.212493
167.349743	5352.903219	25.217511
167.307270	5359.491831	25.222528
167.419007	5365.445361	25.227546
167.607024	5371.105084	25.232563
167.688539	5387.282986	25.237581
168.500926	5387.583912	25.242599
168.676006	5403.035714	25.247616
168.590619	5399.834098	25.252634
168.748604	5403.168342	25.257651
168.893117	5412.199056	25.262669
169.228133	5417.118652	25.267687
169.515124	5419.990977	25.272704
169.540578	5429.131944	25.277722
169.540822	5418.826690	25.282739
169.524993	5430.423320	25.287757
169.981534	5442.537049	25.292775
170.115159	5452.124166	25.297792
169.751043	5454.253006	25.302810
170.146766	5455.497570	25.307827
170.344114	5462.969249	25.312845
170.569155	5466.500513	25.317863
170.504340	5482.409974	25.322880
170.576685	5496.542388	25.327898
170.994195	5504.026189	25.332915
171.315640	5504.986790	25.337933
171.461178	5503.883520	25.342951
171.983000	5505.402220	25.347968
171.551736	5514.827691	25.352986
172.424789	5529.946483	25.358003
172.052255	5527.650520	25.363021
172.183269	5527.704487	25.368039
172.427343	5529.385484	25.373056
172.946638	5542.097434	25.378074
172.849610	5557.756425	25.383091
173.073519	5560.557803	25.388109
173.068695	5559.157515	25.393127
173.428950	5562.645214	25.398144
173.321772	5578.964342	25.403162
173.839659	5579.097451	25.408179
173.881662	5586.467298	25.413197
173.814252	5590.363061	25.418215
174.110657	5599.839354	25.423232
174.044068	5625.793513	25.428250
174.458155	5617.631296	25.433267
174.650597	5619.053832	25.438285
175.054081	5637.997980	25.443303
175.257844	5651.705207	25.448320
175.211244	5646.145791	25.453338
175.655298	5641.644197	25.458355
175.295672	5645.531493	25.463373
175.572210	5681.433638	25.468391
175.937874	5673.057250	25.473408
175.885648	5672.343466	25.478426
176.358648	5675.498521	25.483443
176.661556	5688.621161	25.488461
176.882095	5681.820933	25.493479
177.156142	5679.801851	25.498496
176.577466	5688.104653	25.503514
177.198092	5700.621996	25.508531
177.468106	5707.168808	25.513549
177.398633	5728.905100	25.518567
177.928559	5721.861200	25.523584
177.744236	5721.373028	25.528602
177.917722	5739.260406	25.533619
177.844686	5754.129822	25.538637
178.202842	5743.647691	25.543655
178.449026	5764.225973	25.548672
178.502305	5779.043805	25.553690
178.638000	5773.242855	25.558707
178.975377	5790.566818	25.563725
178.984690	5803.317035	25.568743
179.494139	5797.871887	25.573760
179.628619	5824.575577	25.578778
179.976521	5825.956039	25.583795
180.142992	5833.627158	25.588813
180.540394	5833.602464	25.593831
180.474201	5819.704216	25.598848
180.345794	5844.875574	25.603866
180.638322	5852.889296	25.608883
180.937381	5853.461689	25.613901
180.873932	5857.482770	25.618919
181.142411	5863.914245	25.623936
181.217854	5874.589549	25.628954
181.462780	5875.005356	25.633971
181.776349	5878.126083	25.638989
182.029309	5882.315440	25.644007
182.465466	5897.173051	25.649024
182.266812	5906.121886	25.654042
182.337333	5914.443254	25.659059
182.514555	5911.962020	25.664077
182.593191	5922.706083	25.669095
182.838184	5927.930518	25.674112
182.967874	5925.102821	25.679130
183.427772	5938.336763	25.684148
183.575726	5959.351105	25.689165
183.982341	5971.141222	25.694183
184.048920	5959.678711	25.699200
183.775346	5972.976127	25.704218
183.934155	5972.637794	25.709236
184.459426	5980.047227	25.714253
184.545760	5987.714681	25.719271
184.707212	5987.054143	25.724288
184.651254	6012.840495	25.729306
185.055169	6012.780146	25.734324
185.481116	6016.137895	25.739341
185.232659	6037.985787	25.744359
185.787263	6037.755863	25.749376
185.659846	6052.834087	25.754394
186.039878	6050.942035	25.759412
186.340459	6072.532502	25.764429
186.532967	6086.148303	25.769447
186.995308	6071.168724	25.774464
187.327662	6067.927110	25.779482
187.184380	6073.923159	25.784500
187.581589	6077.903899	25.789517
187.545769	6100.160928	25.794535
187.853079	6105.428204	25.799552
187.854595	6109.140812	25.804570
187.917783	6108.951472	25.809588
188.497614	6117.128025	25.814605
188.228592	6127.194402	25.819623
188.091054	6124.486376	25.824640
188.550190	6122.957777	25.829658
188.712760	6142.689199	25.834676
189.126332	6140.282752	25.839693
189.056959	6155.727899	25.844711
189.148648	6172.460497	25.849728
189.334342	6176.781826	25.854746
189.569843	6192.726781	25.859764
190.254560	6207.588349	25.864781
190.203572	6208.668959	25.869799
190.541406	6204.496482	25.874816
190.249708	6214.569680	25.879834
190.728559	6223.659309	25.884852
190.962857	6225.486713	25.889869
190.971280	6240.813332	25.894887
191.523306	6226.125353	25.899904
191.366400	6252.758258	25.904922
191.420663	6259.961264	25.909940
191.779386	6263.395878	25.914957
191.901152	6271.359164	25.919975
192.017285	6280.498789	25.924992
192.155735	6290.169081	25.930010
192.021535	6292.211025	25.935028
192.439916	6309.521111	25.940045
192.602429	6320.759560	25.945063
193.129560	6338.896551	25.950080
193.243962	6355.565939	25.955098
193.644851	6346.639897	25.960116
193.919146	6346.752064	25.965133
194.167048	6370.909174	25.970151
194.633062	6371.258279	25.975168
194.730702	6380.207368	25.980186
194.838890	6376.855086	25.985204
195.070759	6363.973315	25.990221
194.836719	6374.989429	25.995239
195.045361	6377.673809	26.000256
195.418193	6401.453069	26.005274
195.637905	6389.819471	26.010292
195.892856	6398.393374	26.015309
195.770946	6405.113919	26.020327
196.070591	6410.984414	26.025344
196.194302	6423.368383	26.030362
196.662443	6415.599160	26.035380
196.961764	6434.229707	26.040397
196.755345	6445.098275	26.045415
197.285657	6448.628315	26.050432
197.124975	6445.399136	26.055450
197.242740	6474.152295	26.060468
197.604983	6472.277978	26.065485
197.703672	6487.001161	26.070503
198.088813	6495.822657	26.075520
198.174367	6510.820972	26.080538
197.932842	6519.677089	26.085556
198.396290	6519.028178	26.090573
198.472971	6536.430773	26.095591
198.931873	6537.765287	26.100608
199.585934	6553.763493	26.105626
199.294391	6558.664564	26.110644
199.476769	6543.497831	26.115661
199.828991	6564.175981	26.120679
199.664875	6589.452645	26.125696
199.763376	6590.968934	26.130714
199.883555	6602.575483	26.135732
200.595139	6618.522889	26.140749
200.636429	6631.894220	26.145767
201.162604	6650.303977	26.150784
201.330217	6650.152271	26.155802
201.400340	6649.280458	26.160820
201.608399	6652.864285	26.165837
201.417384	6668.596868	26.170855
201.623465	6673.950513	26.175872
201.979201	6675.819984	26.180890
202.208908	6698.127633	26.185908
202.752661	6696.048109	26.190925
202.672248	6709.808707	26.195943
202.744576	6701.916756	26.200960
203.277270	6725.182451	26.205978
202.991554	6740.870412	26.210996
203.478279	6733.194838	26.216013
203.520282	6745.488247	26.221031
203.810055	6766.344224	26.226048
203.776602	6767.837508	26.231066
204.053564	6783.569564	26.236084
204.590153	6788.674645	26.241101
204.625435	6797.658319	26.246119
204.837428	6816.144337	26.251136
204.919066	6829.722637	26.256154
205.044590	6832.012790	26.261172
205.876626	6847.060810	26.266189
205.970733	6847.883081	26.271207
206.348944	6857.427398	26.276224
206.519397	6846.848531	26.281242
206.305112	6854.892458	26.286260
206.639255	6864.962309	26.291277
207.141996	6878.431031	26.296295
207.012099	6892.331869	26.301312
207.785642	6880.707157	26.306330
207.472589	6904.676829	26.311348
207.603318	6903.991253	26.316365
207.908111	6905.783115	26.321383
208.065048	6904.646455	26.326400
208.198838	6927.539388	26.331418
208.206832	6932.477801	26.336436
208.551409	6937.787432	26.341453
208.695824	6966.665547	26.346471
208.913303	6958.448185	26.351488
209.448350	6979.415640	26.356506
209.320221	6993.087329	26.361524
209.817476	6982.988149	26.366541
209.686589	7005.745580	26.371559
210.159921	7008.586156	26.376576
210.445572	7009.946763	26.381594
210.288898	7021.475822	26.386612
211.002967	7036.199008	26.391629
210.950592	7055.316794	26.396647
210.967664	7046.501096	26.401664
211.642010	7066.210384	26.406682
211.642689	7081.006433	26.411700
211.843440	7079.738459	26.416717
212.040714	7097.235002	26.421735
212.275680	7101.788727	26.426752
212.572980	7102.683265	26.431770
212.225297	7117.764638	26.436788
212.942878	7111.234653	26.441805
212.887766	7128.363899	26.446823
213.122087	7127.764084	26.451840
213.572818	7128.062147	26.456858
213.595733	7141.064702	26.461876
213.904330	7148.157567	26.466893
213.914036	7157.864688	26.471911
214.253251	7160.280549	26.476928
214.476498	7176.462205	26.481946
214.386992	7205.217566	26.486964
214.938592	7190.097533	26.491981
214.929090	7201.917997	26.496999
214.867480	7230.118971	26.502016
215.485776	7220.685658	26.507034
215.702706	7247.668321	26.512052
216.086884	7253.123610	26.517069
215.866316	7262.075178	26.522087
216.023367	7269.366936	26.527104
216.523887	7278.897536	26.532122
216.234421	7296.543513	26.537140
217.004131	7294.489262	26.542157
217.348759	7313.253750	26.547175
217.093987	7333.538765	26.552192
217.537240	7337.828031	26.557210
217.859589	7347.409898	26.562228
218.197209	7359.618133	26.567245
218.458877	7374.034529	26.572263
218.483029	7367.988728	26.577280
218.697147	7384.517484	26.582298
219.187632	7400.679600	26.587316
219.262479	7402.479070	26.592333
219.378116	7417.316139	26.597351
219.249294	7424.662203	26.602368
219.987060	7433.002371	26.607386
220.291817	7452.071601	26.612404
220.306413	7455.596768	26.617421
220.599916	7454.911971	26.622439
220.772921	7466.259775	26.627456
221.142067	7458.933049	26.632474
221.077222	7473.628204	26.637492
221.477023	7482.429073	26.642509
221.834718	7498.589647	26.647527
221.737130	7494.188020	26.652544
222.052393	7509.614958	26.657562
222.116639	7517.663621	26.662580
222.593389	7528.889874	26.667597
222.617516	7541.287507	26.672615
222.687569	7558.942573	26.677632
222.885519	7559.490246	26.682650
222.917054	7583.975746	26.687668
223.479075	7594.836738	26.692685
223.618146	7606.074786	26.697703
223.832137	7619.129129	26.702720
224.230593	7628.753338	26.707738
224.364048	7652.181708	26.712756
225.000602	7650.734054	26.717773
225.143544	7658.563308	26.722791
224.856294	7656.872650	26.727808
225.372785	7648.391646	26.732826
225.192817	7682.918119	26.737844
225.397885	7678.823056	26.742861
226.047236	7697.256188	26.747879
226.108630	7712.082527	26.752896
226.546424	7712.420438	26.757914
226.898252	7728.904806	26.762932
226.904907	7744.462231	26.767949
227.319770	7740.284922	26.772967
227.532291	7751.895748	26.777984
227.850415	7748.286227	26.783002
227.705959	7768.263897	26.788020
227.851018	7766.756101	26.793037
228.428072	7785.547870	26.798055
228.512515	7801.035513	26.803072
228.747501	7790.882394	26.808090
228.758964	7810.198701	26.813108
229.185659	7821.232510	26.818125
229.465434	7816.836724	26.823143
229.492030	7847.581292	26.828160
229.728552	7848.598875	26.833178
229.927256	7854.157135	26.838196
230.015782	7876.957242	26.843213
230.490887	7877.225475	26.848231
230.772577	7889.565814	26.853248
231.069990	7914.893901	26.858266
231.136540	7914.550566	26.863284
231.602709	7923.456001	26.868301
231.627278	7932.731633	26.873319
231.458320	7946.884393	26.878336
232.087598	7949.151855	26.883354
232.130967	7954.483907	26.888372
232.521970	7972.986108	26.893389
232.883621	7994.243883	26.898407
232.872523	8002.344949	26.903424
233.223500	8016.463676	26.908442
233.417585	8026.573958	26.913460
233.935866	8033.838409	26.918477
234.282349	8048.634586	26.923495
234.423615	8051.657353	26.928512
234.754641	8053.064334	26.933530
234.627239	8066.826593	26.938548
234.792843	8071.011621	26.943565
235.409567	8080.054457	26.948583
235.293044	8100.644236	26.953600
235.613044	8102.809948	26.958618
235.922799	8121.725803	26.963636
236.165552	8137.862907	26.968653
236.501348	8141.866597	26.973671
235.925594	8151.476486	26.978688
236.660821	8160.128291	26.983706
237.006732	8167.213338	26.988724
237.006824	8180.448632	26.993741
237.456261	8192.650746	26.998759
237.321567	8200.277467	27.003776
237.701728	8213.143746	27.008794
238.553341	8233.211117	27.013812
238.569651	8235.370967	27.018829
238.816033	8238.653209	27.023847
238.897074	8250.718166	27.028864
239.157926	8257.846718	27.033882
239.059674	8256.885196	27.038900
239.161420	8278.073860	27.043917
239.620200	8290.856855	27.048935
239.956212	8303.135371	27.053952
240.149740	8320.241300	27.058970
240.584733	8329.803487	27.063988
240.688578	8346.586170	27.069005
241.166963	8350.534138	27.074023
241.235702	8361.607315	27.079040
241.647256	8372.329983	27.084058
241.684102	8378.960796	27.089076
241.740379	8381.919277	27.094093
242.207214	8399.692284	27.099111
242.134943	8405.991914	27.104128
242.540791	8426.590935	27.109146
242.889605	8429.302137	27.114164
243.069209	8450.332273	27.119181
243.420313	8443.441522	27.124199
243.482398	8474.414642	27.129216
244.345532	8485.675244	27.134234
244.410089	8500.633274	27.139252
244.459621	8496.633604	27.144269
244.666198	8496.434362	27.149287
244.766148	8515.442787	27.154304
244.973058	8517.193012	27.159322
245.225883	8543.863843	27.164340
245.349757	8551.167816	27.169357
245.809991	8569.145097	27.174375
245.727984	8587.738024	27.179392
246.164008	8585.949663	27.184410
246.535660	8617.884892	27.189428
246.448794	8637.705033	27.194445
247.051937	8644.094606	27.199463
246.971530	8656.583011	27.204480
247.335517	8665.774696	27.209498
247.577536	8681.829096	27.214516
247.615441	8707.720826	27.219533
247.969147	8703.040732	27.224551
248.273184	8731.894859	27.229568
248.467014	8738.745533	27.234586
249.023243	8749.963194	27.239604
248.772581	8766.386196	27.244621
249.402604	8781.151675	27.249639
249.734154	8803.913672	27.254656
249.960205	8813.489807	27.259674
250.378338	8832.695002	27.264692
250.461364	8829.492943	27.269709
250.838435	8836.056347	27.274727
251.271774	8843.271393	27.279744
251.453203	8867.691825	27.284762
251.913698	8859.535016	27.289780
251.814797	8857.087874	27.294797
252.088186	8868.576948	27.299815
252.302335	8881.467124	27.304832
252.420626	8878.832697	27.309850
252.733069	8901.102922	27.314868
252.463834	8911.293171	27.319885
252.875105	8924.954218	27.324903
253.252235	8948.620414	27.329920
253.648313	8943.579381	27.334938
254.024183	8977.748753	27.339956
253.932374	8976.826289	27.344973
254.117907	9003.623558	27.349991
254.539961	9010.773597	27.355008
254.941261	9033.415051	27.360026
255.096197	9040.305115	27.365044
255.072134	9050.867541	27.370061
255.718151	9054.946757	27.375079
256.016031	9075.977413	27.380096
255.964365	9097.683126	27.385114
256.421511	9105.669229	27.390132
256.871196	9137.236654	27.395149
257.094156	9130.652458	27.400167
257.311849	9144.321743	27.405184
257.570150	9155.372766	27.410202
257.998522	9161.557497	27.415220
257.947817	9181.804220	27.420237
258.117236	9194.983123	27.425255
258.305910	9199.849811	27.430272
258.358249	9214.924214	27.435290
259.131738	9235.753373	27.440308
259.392202	9249.668540	27.445325
259.548337	9255.976579	27.450343
259.951302	9279.804044	27.455360
260.104899	9280.139303	27.460378
260.461980	9294.942901	27.465396
260.525879	9317.048763	27.470413
260.983625	9322.925910	27.475431
261.470947	9345.356212	27.480448
261.382568	9356.409528	27.485466
261.631132	9360.134717	27.490484
261.803272	9375.335374	27.495501
262.113367	9384.016718	27.500519
262.120123	9396.974630	27.505536
262.530842	9410.291926	27.510554
262.837752	9431.166223	27.515572
263.152931	9455.469107	27.520589
263.447161	9448.919447	27.525607
263.589706	9474.598695	27.530624
263.589754	9495.265847	27.535642
263.948675	9492.569347	27.540660
264.089323	9505.169199	27.545677
264.680471	9532.313148	27.550695
264.882381	9539.233335	27.555712
265.422602	9557.631486	27.560730
265.754191	9555.853369	27.565748
265.945878	9562.309718	27.570765
266.530198	9569.128041	27.575783
266.698244	9578.268503	27.580800
266.681661	9586.086032	27.585818
267.187728	9587.513664	27.590836
267.407619	9602.789570	27.595853
267.631636	9608.130403	27.600871
267.377160	9610.641311	27.605888
267.903972	9638.327686	27.610906
268.062035	9641.730558	27.615924
268.027028	9666.417763	27.620941
268.601033	9676.606717	27.625959
269.067894	9698.172410	27.630976
269.297144	9705.408999	27.635994
269.821873	9719.079840	27.641012
269.948114	9735.107790	27.646029
269.958763	9745.850107	27.651047
270.014646	9758.018266	27.656064
270.280696	9777.004570	27.661082
270.648208	9787.095093	27.666100
270.563871	9806.743244	27.671117
271.150767	9824.420513	27.676135
271.243555	9839.587466	27.681152
271.350834	9867.163678	27.686170
272.110768	9882.876329	27.691188
272.359813	9898.178580	27.696205
272.826613	9916.175328	27.701223
273.154172	9926.668156	27.706240
273.190494	9927.971598	27.711258
273.861269	9943.774468	27.716276
274.144695	9951.176067	27.721293
274.296308	9961.907873	27.726311
274.761455	9973.829969	27.731328
274.662724	9982.143210	27.736346
275.298540	9996.919208	27.741364
275.587706	10000.539322	27.746381
275.314743	10022.444548	27.751399
275.586222	10036.906817	27.756416
275.622524	10056.652535	27.761434
276.273760	10055.435675	27.766452
276.445278	10093.702513	27.771469
276.748231	10097.303534	27.776487
277.171274	10109.204906	27.781504
277.268246	10145.042565	27.786522
277.719027	10145.605917	27.791540
278.181773	10177.140008	27.796557
278.342103	10173.445287	27.801575
278.603928	10176.768784	27.806592
278.954050	10192.375525	27.811610
279.233615	10200.735222	27.816628
279.411609	10202.192782	27.821645
279.375337	10217.747027	27.826663
279.727947	10236.953063	27.831680
279.809418	10253.318842	27.836698
279.975160	10259.839833	27.841716
280.630186	10290.965764	27.846733
280.631654	10289.844194	27.851751
281.071135	10306.319806	27.856768
281.002027	10326.207811	27.861786
281.368993	10345.763480	27.866804
281.485402	10369.342842	27.871821
281.860344	10371.905830	27.876839
282.521652	10395.985080	27.881856
282.421800	10412.126129	27.886874
282.947552	10429.238572	27.891892
283.326059	10452.185651	27.896909
283.628962	10464.478703	27.901927
283.800935	10481.206879	27.906944
283.906309	10498.185724	27.911962
284.576100	10516.792239	27.916980
284.976137	10535.358353	27.921997
284.807705	10551.067010	27.927015
285.549939	10567.942454	27.932032
285.739731	10582.225848	27.937050
286.110438	10601.045411	27.942068
286.587966	10607.775386	27.947085
286.881865	10611.627848	27.952103
286.991794	10645.033588	27.957120
287.146495	10649.882949	27.962138
287.957387	10658.500166	27.967156
287.781605	10670.609188	27.972173
288.017664	10688.449648	27.977191
288.523670	10698.688705	27.982208
288.716217	10710.032714	27.987226
289.086476	10722.179483	27.992244
289.574382	10735.298746	27.997261
289.675557	10750.053676	28.002279
289.736520	10761.904674	28.007296
289.656204	10771.763065	28.012314
290.327001	10788.891757	28.017332
290.586104	10807.423614	28.022349
290.651360	10832.410372	28.027367
291.290278	10832.786760	28.032384
291.452451	10852.103819	28.037402
291.808924	10875.329724	28.042420
292.384444	10885.841156	28.047437
292.319018	10894.004582	28.052455
292.733311	10915.559158	28.057472
292.750547	10928.602109	28.062490
293.151566	10945.719678	28.067508
293.048919	10964.857545	28.072525
293.417593	10991.701184	28.077543
293.804038	10998.985751	28.082560
294.159141	11026.752823	28.087578
294.381217	11044.928056	28.092596
294.790384	11061.985432	28.097613
295.011353	11075.700817	28.102631
295.570260	11079.487157	28.107648
295.738229	11105.990728	28.112666
296.164878	11110.068500	28.117684
296.435004	11120.511507	28.122701
296.350030	11150.925283	28.127719
297.059667	11153.453558	28.132736
297.330330	11181.500390	28.137754
297.359327	11185.318095	28.142772
297.989410	11196.676945	28.147789
298.256992	11204.841569	28.152807
298.997914	11209.090433	28.157824
298.999951	11240.254335	28.162842
299.350365	11235.864016	28.167860
299.621440	11251.016567	28.172877
299.651608	11270.248165	28.177895
300.337144	11268.808140	28.182912
300.161791	11286.381967	28.187930
300.346469	11298.626075	28.192948
300.800391	11317.877947	28.197965
301.026656	11338.319141	28.202983
301.476900	11348.414848	28.208000
301.441485	11373.712900	28.213018
301.582314	11384.876378	28.218036
302.124319	11402.038107	28.223053
302.230595	11420.131509	28.228071
302.999483	11439.744566	28.233088
303.130331	11466.032346	28.238106
303.354209	11477.820162	28.243124
303.756341	11496.984892	28.248141
303.951365	11508.294478	28.253159
304.448508	11530.831952	28.258176
304.224582	11553.241582	28.263194
304.876209	11571.294680	28.268212
305.534968	11584.687322	28.273229
305.289284	11609.366423	28.278247
306.005100	11624.707799	28.283264
306.348381	11650.797547	28.288282
306.450010	11663.659252	28.293300
307.161395	11678.356791	28.298317
307.172607	11690.710325	28.303335
308.070833	11698.562986	28.308352
307.981073	11721.487073	28.313370
308.316512	11739.822165	28.318388
309.072126	11729.265451	28.323405
308.938111	11767.674565	28.328423
309.235055	11775.586110	28.333440
309.311498	11793.463943	28.338458
309.499674	11801.657290	28.343476
309.933436	11818.355852	28.348493
310.052783	11832.615652	28.353511
310.727315	11851.614833	28.358528
310.719748	11870.322333	28.363546
310.917710	11873.512948	28.368564
311.093405	11885.888240	28.373581
311.514833	11917.598636	28.378599
312.035459	11921.790144	28.383616
312.429813	11947.871478	28.388634
312.392431	11958.958120	28.393652
312.725900	11974.158320	28.398669
313.125863	12005.249945	28.403687
313.571495	12010.121852	28.408704
313.741194	12037.725535	28.413722
314.032011	12043.886760	28.418740
314.555244	12061.333417	28.423757
314.448233	12089.515720	28.428775
314.836317	12103.008833	28.433792
315.298406	12122.244101	28.438810
315.673204	12149.732656	28.443828
315.724680	12167.382721	28.448845
316.122131	12194.929533	28.453863
316.954279	12202.314448	28.458880
317.021155	12219.960940	28.463898
317.095847	12240.500317	28.468916
317.539406	12247.305713	28.473933
317.593250	12281.014442	28.478951
318.266463	12299.619872	28.483968
318.928536	12313.006734	28.488986
319.233804	12327.986874	28.494004
319.714441	12342.472335	28.499021
320.037272	12359.086067	28.504039
320.303926	12361.359700	28.509056
320.408307	12376.209568	28.514074
320.853592	12398.836691	28.519092
321.260156	12390.498877	28.524109
321.316220	12411.024925	28.529127
321.932200	12427.968636	28.534144
322.059032	12439.500336	28.539162
322.334417	12454.338375	28.544180
322.456817	12477.496812	28.549197
322.959738	12497.530661	28.554215
323.167228	12509.644409	28.559232
323.348755	12534.082383	28.564250
323.458954	12553.629108	28.569268
324.003353	12577.129536	28.574285
324.323477	12600.316862	28.579303
324.442984	12624.179064	28.584320
324.842190	12641.740612	28.589338
325.208586	12667.268798	28.594356
325.418572	12675.606135	28.599373
325.834864	12701.667367	28.604391
326.306920	12727.965924	28.609408
326.508259	12737.128581	28.614426
326.826232	12764.812280	28.619444
327.677486	12771.595837	28.624461
327.742411	12802.033110	28.629479
328.137323	12811.382205	28.634496
328.043391	12830.785310	28.639514
328.634672	12849.590827	28.644532
329.062207	12857.405384	28.649549
328.954168	12865.027844	28.654567
329.700987	12892.537168	28.659584
329.988953	12901.846888	28.664602
329.704260	12938.902959	28.669620
330.469064	12942.854143	28.674637
330.829544	12970.003284	28.679655
331.092963	12977.212000	28.684672
331.508017	12999.038235	28.689690
331.680714	13020.910998	28.694708
332.140018	13028.496644	28.699725
332.188804	13051.464413	28.704743
332.623686	13071.496485	28.709760
333.137902	13086.757353	28.714778
332.991961	13114.963110	28.719796
333.366893	13141.101546	28.724813
333.557733	13164.961690	28.729831
333.975707	13195.882867	28.734848
334.344978	13213.412658	28.739866
334.769127	13248.490410	28.744884
335.384280	13259.418707	28.749901
335.788524	13286.592531	28.754919
336.028873	13309.125175	28.759936
336.722170	13323.236067	28.764954
336.560616	13355.444022	28.769972
337.702044	13359.844775	28.774989
337.763570	13381.933544	28.780007
338.353887	13393.673212	28.785024
338.815950	13406.939530	28.790042
338.830763	13413.843011	28.795060
339.201123	13428.516227	28.800077
339.242447	13445.600386	28.805095
339.438094	13465.875667	28.810112
340.178951	13475.496215	28.815130
340.146847	13506.821734	28.820148
340.758953	13508.896932	28.825165
341.047634	13538.037625	28.830183
341.685175	13543.335507	28.835200
341.782137	13569.455222	28.840218
342.319860	13579.859647	28.845236
342.569623	13600.428159	28.850253
342.545443	13622.202397	28.855271
342.966768	13639.496995	28.860288
343.546535	13643.923489	28.865306
343.568830	13668.966044	28.870324
343.908670	13684.463608	28.875341
344.225903	13701.057763	28.880359
344.613336	13731.640023	28.885376
344.835753	13755.579598	28.890394
345.134174	13777.344488	28.895412
345.348183	13791.918208	28.900429
345.464450	13828.091817	28.905447
346.166448	13851.204254	28.910464
346.777858	13876.483579	28.915482
347.069985	13897.969387	28.920500
347.522788	13904.435383	28.925517
347.894369	13917.298287	28.930535
348.207827	13924.889032	28.935552
348.733960	13941.840201	28.940570
348.802853	13961.372489	28.945588
348.931007	13969.717480	28.950605
349.435080	13991.850549	28.955623
349.386845	14015.682430	28.960640
350.407617	14031.128605	28.965658
350.838513	14057.297286	28.970676
350.999156	14065.544067	28.975693
351.112474	14081.631228	28.980711
351.254342	14103.589178	28.985728
351.691866	14133.228303	28.990746
351.685413	14152.705146	28.995764
352.528108	14172.709005	29.000781
352.638007	14197.663879	29.005799
353.012901	14227.636409	29.010816
353.666518	14235.687036	29.015834
353.834664	14265.732537	29.020852
354.206859	14286.289254	29.025869
354.649343	14307.201431	29.030887
355.003271	14312.453276	29.035904
355.257247	14343.872088	29.040922
355.718700	14376.579109	29.045940
356.088393	14384.968883	29.050957
356.190397	14421.892039	29.055975
356.588538	14444.905910	29.060992
356.855615	14450.340202	29.066010
357.155615	14488.181327	29.071028
357.474194	14505.243347	29.076045
357.957771	14542.516610	29.081063
358.435558	14561.545636	29.086080
358.766510	14585.657063	29.091098
358.956630	14611.897120	29.096116
359.653045	14638.670290	29.101133
360.136679	14656.218157	29.106151
360.434710	14681.088046	29.111168
360.860830	14696.122803	29.116186
360.951332	14717.316483	29.121204
361.361795	14736.422975	29.126221
361.750551	14758.944051	29.131239
362.131471	14787.197441	29.136256
362.873919	14806.891025	29.141274
363.039736	14823.289521	29.146292
363.671296	14839.045343	29.151309
363.859449	14868.277610	29.156327
364.035913	14884.514669	29.161344
364.845082	14911.221345	29.166362
365.028906	14918.765546	29.171380
365.246773	14949.655061	29.176397
365.408685	14958.464005	29.181415
365.713031	14992.209260	29.186432
366.388890	15002.280615	29.191450
366.458923	15025.015043	29.196468
367.094669	15036.910820	29.201485
367.331959	15043.291500	29.206503
367.341745	15076.242530	29.211520
367.977513	15096.708838	29.216538
367.851875	15117.436540	29.221556
368.574248	15127.063947	29.226573
369.092873	15146.922156	29.231591
369.518190	15164.445066	29.236608
370.303826	15181.413438	29.241626
370.263743	15206.397892	29.246644
371.009716	15213.452936	29.251661
371.237693	15231.497525	29.256679
371.191018	15248.044193	29.261696
371.775218	15265.602715	29.266714
371.690432	15280.931923	29.271732
372.392751	15314.834995	29.276749
373.034382	15335.055857	29.281767
373.152802	15356.957248	29.286784
373.703234	15370.416181	29.291802
373.581189	15406.574519	29.296820
374.135905	15428.287118	29.301837
374.744168	15445.029276	29.306855
374.996514	15470.384015	29.311872
375.294349	15483.321498	29.316890
375.699004	15502.702364	29.321908
376.023400	15517.162816	29.326925
376.550900	15558.016018	29.331943
376.489032	15587.753488	29.336960
377.113280	15592.579406	29.341978
377.126705	15631.075603	29.346996
377.450286	15667.660499	29.352013
378.176836	15683.325104	29.357031
378.220830	15714.814731	29.362048
378.515655	15744.610209	29.367066
379.297662	15775.760150	29.372084
379.552167	15801.541789	29.377101
380.192595	15831.011640	29.382119
380.587275	15852.016805	29.387136
381.126883	15870.869333	29.392154
381.640003	15895.461782	29.397172
382.108200	15921.787922	29.402189
382.444541	15932.917874	29.407207
382.626639	15957.856826	29.412224
383.363711	15987.106885	29.417242
383.483798	15995.443048	29.422260
383.937113	16016.071435	29.427277
384.521828	16035.396432	29.432295
385.016905	16061.550837	29.437312
385.271405	16057.875914	29.442330
385.439147	16081.231179	29.447348
385.272076	16106.975309	29.452365
386.111524	16126.095679	29.457383
386.229607	16154.670598	29.462400
386.904345	16181.346892	29.467418
387.169241	16200.008990	29.472436
387.408314	16218.485882	29.477453
387.646538	16241.936444	29.482471
387.810704	16276.858076	29.487488
388.210508	16291.365306	29.492506
388.385438	16319.807473	29.497524
388.726296	16357.288379	29.502541
389.184616	16381.420914	29.507559
389.388208	16420.492735	29.512576
389.685820	16442.420160	29.517594
390.631764	16477.135594	29.522612
391.205179	16508.715391	29.527629
391.414806	16528.820179	29.532647
391.871947	16564.581693	29.537664
392.320125	16573.383740	29.542682
392.515326	16598.151189	29.547700
392.553817	16639.218145	29.552717
393.276557	16657.100047	29.557735
394.125972	16684.542204	29.562752
394.217853	16714.745972	29.567770
394.404810	16740.949648	29.572788
394.997199	16769.607786	29.577805
395.417142	16799.092782	29.582823
395.932742	16828.617507	29.587840
396.712282	16845.241889	29.592858
396.977541	16871.987191	29.597876
397.389640	16905.995040	29.602893
397.887524	16916.916912	29.607911
398.174598	16951.156574	29.612928
398.628203	16975.112659	29.617946
398.957193	16997.448040	29.622964
399.375376	17022.247955	29.627981
400.021882	17040.205833	29.632999
399.906370	17065.206793	29.638016
400.725209	17081.298641	29.643034
400.740619	17108.198131	29.648052
400.849739	17133.176594	29.653069
401.617667	17166.211858	29.658087
401.767463	17187.306880	29.663104
402.464910	17219.019736	29.668122
403.147522	17244.956326	29.673140
403.285933	17269.790393	29.678157
404.002955	17291.514607	29.683175
404.123542	17333.526554	29.688192
404.526713	17343.010185	29.693210
405.155270	17364.858631	29.698228
405.007091	17398.803113	29.703245
405.761949	17406.219263	29.708263
406.075316	17443.653451	29.713280
406.496003	17454.866731	29.718298
406.650473	17493.464083	29.723316
407.086634	17510.722805	29.728333
407.652318	17541.844365	29.733351
407.818335	17577.692408	29.738368
408.660156	17598.358842	29.743386
408.909178	17626.398913	29.748404
408.920649	17651.898274	29.753421
409.718925	17673.431547	29.758439
409.981344	17698.379606	29.763456
410.404155	17708.851626	29.768474
410.755498	17745.285853	29.773492
411.252869	17760.751715	29.778509
411.891078	17787.686409	29.783527
412.168688	17808.055247	29.788544
412.633162	17831.595396	29.793562
412.840808	17851.072323	29.798580
413.221195	17892.662317	29.803597
413.796958	17903.638820	29.808615
413.915210	17918.486138	29.813632
414.419568	17951.644607	29.818650
414.958545	17977.817909	29.823668
415.419326	18010.655111	29.828685
415.897411	18036.937819	29.833703
416.691755	18057.121502	29.838720
416.486976	18074.817620	29.843738
417.252335	18100.833014	29.848756
417.060528	18132.049295	29.853773
417.462425	18165.644226	29.858791
418.248035	18186.789297	29.863808
418.713049	18219.375090	29.868826
419.033565	18239.885689	29.873844
419.238903	18280.079039	29.878861
420.001580	18292.979958	29.883879
420.264909	18333.785855	29.888896
420.879540	18352.276917	29.893914
421.145505	18375.575903	29.898932
421.688897	18417.221644	29.903949
422.280886	18435.622712	29.908967
422.786400	18465.853750	29.913984
423.103805	18498.466405	29.919002
423.442188	18516.498921	29.924020
423.790648	18547.528769	29.929037
424.530521	18561.842613	29.934055
424.735739	18602.234456	29.939072
424.979186	18620.340094	29.944090
425.730111	18642.495660	29.949108
425.949575	18673.593952	29.954125
426.482386	18703.040775	29.959143
426.834700	18723.328439	29.964160
426.909598	18755.957045	29.969178
427.446767	18786.180907	29.974196
428.004103	18816.574454	29.979213
428.342909	18833.986390	29.984231
428.581174	18872.242903	29.989248
429.428680	18894.337771	29.994266
430.229695	18922.976507	29.999284
430.070606	18962.353279	30.004301
430.734476	18982.505417	30.009319
431.012955	19001.623278	30.014336
431.385104	19044.720873	30.019354
431.749737	19070.944274	30.024372
431.815659	19080.311444	30.029389
432.219107	19110.400543	30.034407
432.944700	19147.655241	30.039424
433.325586	19175.066047	30.044442
433.958144	19195.987662	30.049460
434.129918	19228.087228	30.054477
434.809954	19268.019690	30.059495
435.264055	19281.597017	30.064512
435.783850	19312.390844	30.069530
436.369053	19331.341728	30.074548
436.487216	19359.877066	30.079565
436.822269	19392.843529	30.084583
437.402219	19416.074360	30.089600
437.523798	19446.808664	30.094618
437.944462	19469.275926	30.099636
438.277663	19512.429055	30.104653
438.750929	19546.145922	30.109671
439.305773	19573.018257	30.114688
440.070182	19608.056294	30.119706
440.423836	19628.830790	30.124724
440.686240	19673.567420	30.129741
441.302323	19701.071216	30.134759
441.693490	19735.067735	30.139776
441.801762	19769.994911	30.144794
442.711798	19790.886899	30.149812
442.979081	19827.008266	30.154829
443.476820	19856.858173	30.159847
443.931808	19890.031795	30.164864
444.363393	19919.337979	30.169882
444.969985	19941.583761	30.174900
445.088176	19982.381662	30.179917
446.271071	19996.706576	30.184935
446.989837	20012.474096	30.189952
447.348962	20042.195246	30.194970
448.300680	20057.760719	30.199988
448.138093	20091.346977	30.205005
448.505795	20101.934137	30.210023
449.503394	20125.427080	30.215040
449.784108	20147.368345	30.220058
451.297972	20126.123782	30.225076
451.789830	20145.266143	30.230093
452.237196	20134.724935	30.235111
452.757910	20133.505744	30.240128
452.673551	20140.741746	30.245146
453.492978	20155.227882	30.250164
453.453752	20172.744859	30.255181
453.606539	20178.345673	30.260199
454.047006	20188.098766	30.265216
453.949982	20205.919116	30.270234
454.254565	20226.125390	30.275252
454.452264	20258.322562	30.280269
454.931323	20279.669354	30.285287
455.029862	20315.843149	30.290304
455.259369	20350.243977	30.295322
455.788669	20372.909434	30.300340
455.867664	20411.653813	30.305357
456.140032	20436.429458	30.310375
456.648424	20477.257045	30.315392
457.028507	20517.059371	30.320410
457.810888	20553.302345	30.325428
458.071790	20610.206940	30.330445
458.768694	20632.156604	30.335463
459.302170	20666.954642	30.340480
459.185887	20716.408798	30.345498
460.235900	20739.282813	30.350516
460.946697	20786.910287	30.355533
461.433465	20807.677746	30.360551
461.781746	20844.061038	30.365568
462.121406	20877.526433	30.370586
462.942183	20903.582588	30.375604
463.117173	20938.251699	30.380621
463.869262	20970.051326	30.385639
464.335238	21006.357967	30.390656
464.419466	21034.726537	30.395674
464.907454	21065.958097	30.400692
465.366202	21108.304941	30.405709
465.960400	21149.485238	30.410727
466.221597	21176.468152	30.415744
467.033701	21207.101804	30.420762
467.539448	21247.089147	30.425780
467.866237	21284.101406	30.430797
468.572882	21317.188739	30.435815
468.913576	21340.512928	30.440832
469.372737	21378.571448	30.445850
469.897355	21403.503745	30.450868
470.485671	21435.188650	30.455885
470.906862	21468.090239	30.460903
471.697561	21502.927122	30.465920
471.858295	21535.858535	30.470938
472.529229	21560.392893	30.475956
473.126440	21598.288979	30.480973
473.474100	21638.122152	30.485991
474.111077	21650.194155	30.491008
474.357424	21687.412344	30.496026
474.751004	21710.537279	30.501044
475.049387	21746.362774	30.506061
475.511372	21781.405432	30.511079
476.122855	21809.992252	30.516096
476.843143	21854.442421	30.521114
477.398273	21886.054766	30.526132
477.519048	21909.468391	30.531149
477.926227	21945.198248	30.536167
478.765476	21966.779787	30.541184
478.816736	22016.842182	30.546202
479.181565	22039.292497	30.551220
479.990480	22073.655982	30.556237
480.345756	22110.586099	30.561255
480.839842	22144.968393	30.566272
481.174822	22179.459593	30.571290
481.846879	22201.138187	30.576308
482.137425	22237.800895	30.581325
482.567657	22269.359873	30.586343
483.120851	22302.714734	30.591360
483.434720	22321.255279	30.596378
483.853184	22364.504269	30.601396
483.956265	22391.378988	30.606413
484.853398	22437.198258	30.611431
485.218948	22457.354768	30.616448
485.660662	22505.956148	30.621466
485.949302	22538.144678	30.626484
486.608137	22582.354657	30.631501
487.079325	22624.420056	30.636519
487.728361	22657.667462	30.641536
488.042779	22704.901957	30.646554
488.703366	22732.950991	30.651572
489.137926	22766.592735	30.656589
489.261044	22811.065125	30.661607
490.166059	22849.919403	30.666624
490.831479	22891.562335	30.671642
491.288101	22929.903824	30.676660
491.846677	22961.312994	30.681677
492.243162	22994.873862	30.686695
493.233243	23026.594846	30.691712
493.594762	23059.043771	30.696730
494.369784	23085.883512	30.701748
495.273244	23114.853086	30.706765
495.619445	23138.551613	30.711783
496.529553	23162.380880	30.716800
496.946953	23187.637114	30.721818
497.391621	23194.942645	30.726836
497.629486	23214.346999	30.731853
497.759980	23245.200330	30.736871
498.519930	23269.093850	30.741888
498.798791	23298.930430	30.746906
499.305911	23327.201092	30.751924
499.702704	23360.333421	30.756941
499.884145	23395.148677	30.761959
500.625963	23431.780070	30.766976
500.705861	23465.524697	30.771994
501.533521	23493.828873	30.777012
502.305005	23545.777285	30.782029
501.890825	23570.692433	30.787047
502.904767	23603.262237	30.792064
503.392056	23638.241972	30.797082
504.013710	23684.826309	30.802100
504.645574	23723.321392	30.807117
505.024190	23756.968640	30.812135
505.487041	23793.330243	30.817152
505.829110	23834.400970	30.822170
506.416870	23856.118902	30.827188
506.857459	23909.004197	30.832205
507.490523	23948.163645	30.837223
507.871682	23974.283113	30.842240
508.163419	24020.302662	30.847258
508.885489	24052.500053	30.852276
509.560089	24077.928622	30.857293
510.108862	24104.639936	30.862311
510.367863	24137.555594	30.867328
510.233556	24174.918249	30.872346
510.968209	24217.579999	30.877364
511.612719	24239.429626	30.882381
511.835415	24291.696331	30.887399
512.678352	24331.397522	30.892416
513.053890	24367.286763	30.897434
513.402071	24401.590076	30.902452
514.195552	24444.916549	30.907469
514.513169	24488.640327	30.912487
515.045782	24533.721856	30.917504
515.558283	24576.074940	30.922522
515.881917	24604.540165	30.927540
516.569641	24654.411812	30.932557
517.044741	24701.794434	30.937575
517.950543	24738.530333	30.942592
518.504584	24781.911621	30.947610
518.842651	24831.562244	30.952628
519.572737	24857.856020	30.957645
520.073530	24897.072749	30.962663
520.494533	24936.667789	30.967680
520.761457	24977.290250	30.972698
521.070282	25020.834134	30.977716
521.686232	25065.129551	30.982733
522.214728	25121.414964	30.987751
523.130668	25162.524525	30.992768
523.111965	25205.492471	30.997786
523.816958	25251.397753	31.002804
524.355903	25299.244623	31.007821
525.066722	25338.793707	31.012839
525.822910	25387.085973	31.017856
526.410163	25434.312685	31.022874
526.851428	25470.298708	31.027892
527.592956	25503.924923	31.032909
527.751716	25552.266377	31.037927
528.488083	25583.880864	31.042944
529.308225	25637.384176	31.047962
529.492353	25673.119356	31.052980
530.211211	25700.533361	31.057997
530.787178	25757.512986	31.063015
531.217770	25776.486428	31.068032
531.897334	25835.162435	31.073050
532.147934	25864.890944	31.078068
532.763560	25907.301245	31.083085
533.288564	25952.963855	31.088103
533.802646	25984.430204	31.093120
534.730435	26018.785677	31.098138
535.287510	26049.075451	31.103156
535.843401	26088.542356	31.108173
535.799936	26129.672522	31.113191
536.637071	26155.043072	31.118208
537.144752	26201.147946	31.123226
537.621487	26236.338315	31.128244
538.516961	26272.959653	31.133261
538.795596	26299.590843	31.138279
539.334918	26332.207185	31.143296
539.784128	26364.836371	31.148314
540.203441	26386.185966	31.153332
540.585328	26434.726150	31.158349
541.252074	26484.614729	31.163367
541.506614	26504.712912	31.168384
542.380237	26533.895162	31.173402
542.476881	26585.365390	31.178420
543.414294	26623.685668	31.183437
543.606782	26665.239699	31.188455
544.138158	26700.088349	31.193472
544.836696	26749.805672	31.198490
545.174518	26791.332940	31.203508
545.916166	26827.401792	31.208525
546.239207	26874.108390	31.213543
546.640088	26928.339839	31.218560
547.313121	26971.212566	31.223578
547.704990	27029.263597	31.228596
548.382381	27081.533154	31.233613
548.660318	27126.476623	31.238631
549.272372	27178.114815	31.243648
550.150159	27223.211176	31.248666
550.477225	27278.598715	31.253684
551.397335	27327.237065	31.258701
551.766180	27373.450139	31.263719
552.452399	27404.998214	31.268736
553.160282	27441.859307	31.273754
553.745724	27503.100365	31.278772
554.744122	27537.715721	31.283789
555.182502	27575.768740	31.288807
555.738069	27619.554545	31.293824
556.361740	27662.254980	31.298842
556.850481	27702.739492	31.303860
557.426706	27736.149334	31.308877
558.078262	27787.050474	31.313895
558.698103	27824.501609	31.318912
559.488541	27855.657368	31.323930
559.583402	27893.863547	31.328948
560.376884	27935.179368	31.333965
560.767978	27971.097835	31.338983
560.904257	28020.361063	31.344000
561.746676	28052.741164	31.349018
562.077953	28101.797096	31.354036
562.748840	28148.049370	31.359053
563.346152	28196.297393	31.364071
564.164873	28236.314680	31.369088
564.534865	28269.778961	31.374106
564.934002	28327.976899	31.379124
565.695421	28351.492532	31.384141
566.471114	28401.367332	31.389159
566.859711	28452.170628	31.394176
567.571012	28472.905260	31.399194
568.094489	28516.188049	31.404212
568.917879	28547.948158	31.409229
569.258711	28582.557039	31.414247
569.820649	28614.325829	31.419264
570.075390	28657.585615	31.424282
570.319998	28686.672623	31.429300
570.988618	28727.816534	31.434317
571.411629	28778.170989	31.439335
572.055555	28818.600486	31.444352
572.559701	28860.445387	31.449370
572.802518	28914.398235	31.454388
573.514686	28965.859158	31.459405
574.137060	29020.505161	31.464423
574.817832	29060.491305	31.469440
575.508044	29102.174822	31.474458
575.472986	29161.317932	31.479476
576.714421	29198.282433	31.484493
577.432960	29242.585622	31.489511
578.026632	29287.844892	31.494528
578.494066	29331.217576	31.499546
579.068249	29383.867955	31.504564
580.015386	29411.563174	31.509581
580.475813	29472.945058	31.514599
580.755687	29503.997784	31.519616
581.852023	29549.265973	31.524634
581.901139	29597.756765	31.529652
582.885891	29637.393343	31.534669
583.055932	29678.609619	31.539687
583.835681	29726.194892	31.544704
584.407556	29772.538489	31.549722
585.250427	29822.928594	31.554740
585.973489	29865.374741	31.559757
586.176172	29934.657024	31.564775
586.680181	29971.876272	31.569792
587.439369	30010.046234	31.574810
587.807622	30067.169492	31.579828
588.597885	30106.253512	31.584845
589.145347	30156.398570	31.589863
589.784454	30203.039997	31.594880
590.144844	30247.480188	31.599898
590.867486	30300.448720	31.604916
591.486294	30347.098520	31.609933
592.000283	30380.304666	31.614951
592.507280	30443.794606	31.619968
593.313081	30488.913112	31.624986
593.650167	30544.068281	31.630004
594.270995	30590.140061	31.635021
594.805546	30640.197254	31.640039
595.431744	30690.446462	31.645056
596.372502	30741.529872	31.650074
596.649429	30795.560737	31.655092
597.612082	30841.786823	31.660109
597.985493	30886.221949	31.665127
598.813246	30942.433483	31.670144
599.659095	30962.620329	31.675162
600.175347	31018.290719	31.680180
600.494285	31046.829520	31.685197
601.067585	31092.363398	31.690215
601.609389	31131.476838	31.695232
602.546455	31157.461894	31.700250
602.617226	31218.691749	31.705268
603.245580	31265.735091	31.710285
603.586366	31305.484595	31.715303
604.056202	31365.056456	31.720320
605.131591	31396.840321	31.725338
605.573346	31437.439334	31.730356
606.073372	31502.966066	31.735373
606.516104	31543.319315	31.740391
607.284922	31592.924447	31.745408
607.890576	31635.018783	31.750426
608.445199	31699.057641	31.755444
609.119041	31732.603581	31.760461
609.881882	31787.597411	31.765479
610.115370	31848.425429	31.770496
611.135389	31892.804438	31.775514
611.768439	31952.489560	31.780532
612.348489	32001.413577	31.785549
612.894407	32045.446098	31.790567
613.575632	32094.916964	31.795584
613.983241	32146.685452	31.800602
614.653816	32206.148010	31.805620
615.131126	32255.692814	31.810637
616.020078	32309.194594	31.815655
616.208879	32365.137634	31.820672
617.360682	32414.219285	31.825690
618.119653	32475.155074	31.830708
618.912455	32520.530286	31.835725
619.324792	32571.317391	31.840743
619.726299	32620.054167	31.845760
620.837071	32662.431643	31.850778
621.003053	32718.500884	31.855796
621.565777	32765.436029	31.860813
622.184696	32817.076823	31.865831
622.821206	32880.221402	31.870848
623.584057	32925.484284	31.875866
624.161708	32984.283519	31.880884
624.453581	33044.078945	31.885901
625.720962	33085.545150	31.890919
625.994404	33146.195052	31.895936
626.380348	33189.009293	31.900954
627.335663	33257.779055	31.905972
627.555681	33307.070079	31.910989
628.440197	33351.428895	31.916007
629.033504	33407.465521	31.921024
629.888196	33463.794882	31.926042
630.684580	33522.320028	31.931060
631.338053	33568.448557	31.936077
632.112009	33624.045738	31.941095
632.406979	33673.026419	31.946112
633.425781	33718.296429	31.951130
633.638240	33767.980951	31.956148
634.323664	33808.803941	31.961165
634.990997	33851.193618	31.966183
635.436003	33898.109743	31.971200
636.303128	33936.899036	31.976218
636.884154	33979.599135	31.981236
637.371392	34010.542239	31.986253
637.867609	34056.195897	31.991271
638.325042	34110.147404	31.996288
639.432981	34152.142961	32.001306
639.757237	34212.170745	32.006324
640.619074	34259.018361	32.011341
641.276977	34309.593569	32.016359
641.639203	34358.874531	32.021376
642.412414	34402.158320	32.026394
642.942919	34461.131097	32.031412
643.395366	34525.129398	32.036429
643.968136	34570.542130	32.041447
644.433446	34618.749693	32.046464
645.288202	34683.761213	32.051482
645.898326	34746.448920	32.056500
646.471568	34802.242807	32.061517
647.625174	34862.555466	32.066535
647.805300	34925.572428	32.071552
648.699554	34970.167343	32.076570
649.735492	35027.836764	32.081588
650.466632	35086.931147	32.086605
651.032783	35132.573473	32.091623
651.410426	35193.010896	32.096640
652.269471	35226.977430	32.101658
653.250872	35290.998490	32.106676
653.807686	35340.959200	32.111693
654.697109	35381.859199	32.116711
654.995883	35447.323246	32.121728
655.440802	35493.252289	32.126746
655.902479	35550.724896	32.131764
656.792930	35609.787882	32.136781
657.415159	35655.454241	32.141799
658.112098	35727.042113	32.146816
658.994408	35772.610624	32.151834
659.598203	35830.219212	32.156852
659.914501	35880.230870	32.161869
660.652124	35936.981391	32.166887
661.279598	36003.046372	32.171904
662.137901	36048.089748	32.176922
662.872191	36108.680216	32.181940
663.424837	36155.174086	32.186957
664.179680	36220.336785	32.191975
664.636199	36274.596562	32.196992
665.677655	36329.032963	32.202010
666.230830	36383.362835	32.207028
666.739010	36441.849553	32.212045
667.646475	36487.564207	32.217063
668.094029	36545.578512	32.222080
668.853345	36601.547431	32.227098
669.418258	36650.426081	32.232116
670.239908	36700.608820	32.237133
670.974707	36745.727346	32.242151
671.388016	36792.853737	32.247168
672.024969	36829.867042	32.252186
672.800842	36887.872821	32.257204
673.206833	36932.552307	32.262221
673.956751	36985.571022	32.267239
674.439692	37035.561169	32.272256
675.116588	37097.034642	32.277274
675.802873	37138.133682	32.282292
676.461353	37207.821559	32.287309
676.597239	37264.066963	32.292327
677.138640	37333.849682	32.297344
678.300793	37395.191796	32.302362
678.582637	37446.999953	32.307380
679.377307	37530.767504	32.312397
680.376528	37591.511920	32.317415
681.134030	37656.501608	32.322432
681.688455	37705.351887	32.327450
682.523218	37772.731004	32.332468
683.128012	37830.235931	32.337485
683.864542	37881.468484	32.342503
684.473284	37955.165871	32.347520
685.270307	38020.650485	32.352538
685.976703	38083.081500	32.357556
686.571268	38143.797738	32.362573
687.509251	38214.913201	32.367591
688.419904	38269.573815	32.372608
689.046084	38325.506602	32.377626
689.899757	38388.938600	32.382644
690.305573	38443.823644	32.387661
691.420003	38501.311206	32.392679
692.004542	38550.167020	32.397696
692.762151	38606.485037	32.402714
693.416892	38657.351393	32.407732
693.604412	38727.755974	32.412749
694.868883	38777.153814	32.417767
695.265688	38849.411404	32.422784
695.803658	38902.356370	32.427802
696.693516	38963.987224	32.432820
697.297541	39026.460098	32.437837
698.253435	39074.257030	32.442855
698.630522	39155.473744	32.447872
698.879801	39214.829670	32.452890
699.942225	39265.025865	32.457908
700.459917	39349.958193	32.462925
701.362971	39411.352049	32.467943
702.218722	39476.692612	32.472960
702.683374	39537.324153	32.477978
703.503550	39590.078109	32.482996
703.741056	39668.519007	32.488013
704.609702	39720.505604	32.493031
705.658729	39799.696213	32.498048
706.287903	39862.311653	32.503066
707.093308	39916.544934	32.508084
707.614553	39976.437356	32.513101
708.563500	40018.870328	32.518119
709.229643	40079.686179	32.523136
709.992676	40141.494462	32.528154
710.703888	40184.530232	32.533172
711.019855	40243.875975	32.538189
711.705216	40284.214860	32.543207
712.532739	40350.559888	32.548224
713.200445	40421.355486	32.553242
714.117200	40474.448467	32.558260
714.681925	40543.639879	32.563277
715.639734	40599.823828	32.568295
716.150221	40655.134587	32.573312
716.654731	40714.578104	32.578330
717.253390	40787.795806	32.583348
717.792379	40854.125654	32.588365
719.166799	40907.278005	32.593383
719.640220	40984.285460	32.598400
720.115763	41043.299485	32.603418
720.710041	41109.634137	32.608436
721.493450	41178.862692	32.613453
722.498104	41236.821713	32.618471
723.441593	41323.416591	32.623488
723.671362	41393.942153	32.628506
724.965891	41445.065084	32.633524
725.595826	41502.983737	32.638541
726.161847	41576.452872	32.643559
726.848262	41641.188416	32.648576
727.419300	41716.918833	32.653594
728.198954	41775.890119	32.658612
728.886227	41847.965921	32.663629
730.188075	41904.094654	32.668647
730.882180	41973.227089	32.673664
731.545482	42047.155873	32.678682
732.642955	42111.190608	32.683700
733.067912	42175.484050	32.688717
733.924081	42229.442181	32.693735
734.623446	42291.869248	32.698752
735.384002	42363.831460	32.703770
735.989567	42425.498008	32.708788
736.651290	42494.470521	32.713805
737.132091	42556.709395	32.718823
738.055358	42638.393493	32.723840
738.663491	42706.044284	32.728858
740.173445	42759.915768	32.733876
740.213469	42839.580747	32.738893
741.126702	42882.299369	32.743911
741.788725	42959.484373	32.748928
742.650567	43033.272229	32.753946
743.344639	43090.246027	32.758964
743.860565	43167.060924	32.763981
744.674513	43234.595854	32.768999
745.554160	43301.149038	32.774016
746.144991	43380.290360	32.779034
746.898340	43433.716615	32.784052
747.289140	43500.562892	32.789069
748.071504	43551.925055	32.794087
748.571866	43624.019118	32.799104
749.233398	43698.314872	32.804122
750.307226	43745.438931	32.809140
750.829817	43831.914707	32.814157
751.731064	43901.536079	32.819175
752.742925	43967.430418	32.824192
753.472388	44046.019601	32.829210
754.150963	44095.765859	32.834228
754.694207	44163.297040	32.839245
755.612561	44227.986448	32.844263
756.232318	44302.802483	32.849280
756.752224	44374.906021	32.854298
758.164677	44443.776265	32.859316
758.623425	44514.918505	32.864333
759.259915	44593.976081	32.869351
760.192716	44651.614187	32.874368
760.849717	44740.265562	32.879386
761.652738	44798.653541	32.884404
762.547969	44871.352404	32.889421
763.357634	44948.030635	32.894439
763.996254	45022.666949	32.899456
764.405906	45091.841366	32.904474
765.791178	45172.454368	32.909492
766.567446	45245.552301	32.914509
767.182982	45321.922370	32.919527
768.040835	45387.244059	32.924544
768.566839	45460.045171	32.929562
769.573875	45532.227386	32.934580
769.718242	45604.152878	32.939597
771.094251	45689.035046	32.944615
771.950845	45756.304843	32.949632
772.214333	45842.437502	32.954650
773.197779	45910.978034	32.959668
773.957885	45997.546643	32.964685
774.805039	46072.990296	32.969703
775.816758	46155.405655	32.974720
776.670183	46226.296443	32.979738
777.532324	46298.776217	32.984756
778.083797	46370.021682	32.989773
778.752165	46450.227838	32.994791
779.617040	46512.426055	32.999808
780.208990	46609.849163	33.004826
781.463143	46665.120704	33.009844
781.924180	46737.864909	33.014861
782.409076	46818.824454	33.019879
783.532737	46898.089396	33.024896
784.149622	46976.245912	33.029914
785.105269	47057.475522	33.034932
785.746865	47140.102719	33.039949
786.442831	47208.135643	33.044967
787.638556	47292.877606	33.049984
788.017412	47354.616652	33.055002
788.830684	47428.553917	33.060020
789.805785	47495.152105	33.065037
790.251072	47565.930276	33.070055
791.274857	47635.190508	33.075072
792.032311	47702.537195	33.080090
792.675298	47778.184748	33.085108
793.434133	47852.078820	33.090125
794.067008	47922.109173	33.095143
795.310312	47996.494672	33.100160
795.813301	48071.077211	33.105178
797.049794	48149.648301	33.110196
797.552792	48211.903826	33.115213
798.176558	48284.675846	33.120231
799.002395	48361.864973	33.125248
799.590373	48434.643307	33.130266
800.764533	48509.117703	33.135284
801.133696	48605.328331	33.140301
802.161297	48671.408285	33.145319
803.260627	48755.768742	33.150336
803.740568	48833.280037	33.155354
804.770807	48907.722225	33.160372
805.570975	48984.429068	33.165389
806.035053	49071.198750	33.170407
807.627876	49141.257836	33.175424
808.169821	49220.988695	33.180442
808.916357	49295.177902	33.185460
809.926770	49376.305339	33.190477
810.705996	49444.122206	33.195495
811.711764	49513.821821	33.200512
812.039651	49601.136428	33.205530
813.074364	49677.534404	33.210548
814.061286	49749.932772	33.215565
814.465397	49833.935687	33.220583
815.559066	49899.924507	33.225600
816.086568	49995.432701	33.230618
816.891442	50070.054484	33.235636
817.679392	50146.907138	33.240653
818.776340	50235.705498	33.245671
819.694729	50309.085828	33.250688
820.202606	50401.074462	33.255706
820.801303	50478.728652	33.260724
822.044592	50557.861582	33.265741
823.083965	50636.572898	33.270759
824.275569	50706.528464	33.275776
825.060711	50774.766015	33.280794
825.686349	50856.630457	33.285812
826.598930	50916.700141	33.290829
827.402268	51007.316296	33.295847
828.380366	51067.372903	33.300864
829.154785	51155.596020	33.305882
829.803385	51224.892122	33.310900
830.912913	51294.178246	33.315917
831.834745	51372.958853	33.320935
832.412654	51452.611912	33.325952
833.123423	51520.198260	33.330970
834.101096	51580.351333	33.335988
834.827445	51648.386975	33.341005
835.137755	51716.208217	33.346023
835.942147	51788.672311	33.351040
836.553099	51857.740159	33.356058
837.386439	51944.916329	33.361076
838.243724	52013.696251	33.366093
838.953079	52100.738269	33.371111
839.952267	52169.663469	33.376128
840.255068	52260.596008	33.381146
841.373113	52338.696336	33.386164
842.528741	52435.073833	33.391181
842.958060	52512.476592	33.396199
844.272328	52591.667180	33.401216
844.911359	52683.599303	33.406234
845.646763	52756.507501	33.411252
846.511562	52842.347992	33.416269
847.486138	52930.781518	33.421287
848.340309	53009.936710	33.426304
849.149101	53106.688613	33.431322
850.489558	53172.808031	33.436340
851.112170	53265.010844	33.441357
852.090685	53343.832093	33.446375
853.033342	53420.895082	33.451392
853.902516	53498.954832	33.456410
854.375647	53595.115748	33.461428
855.493355	53664.674829	33.466445
856.111060	53756.338052	33.471463
856.837272	53840.194807	33.476480
857.751696	53936.662897	33.481498
858.386822	54017.978383	33.486516
859.529752	54103.632249	33.491533
860.232645	54214.837582	33.496551
861.682678	54287.742377	33.501568
862.557492	54380.778720	33.506586
863.351944	54459.331107	33.511604
864.570299	54546.067163	33.516621
865.320216	54631.079037	33.521639
866.086592	54709.655913	33.526656
867.052075	54794.223907	33.531674
867.810720	54867.884980	33.536692
869.137117	54950.679158	33.541709
869.373243	55046.576140	33.546727
870.309530	55114.379932	33.551744
871.258591	55207.850595	33.556762
871.987935	55294.500750	33.561780
873.116382	55380.709016	33.566797
873.819990	55463.825599	33.571815
874.613743	55542.316482	33.576832
875.572114	55634.064364	33.581850
876.729135	55702.927392	33.586868
878.131824	55777.562882	33.591885
878.701943	55869.364266	33.596903
879.914704	55928.427457	33.601920
880.906743	55998.823568	33.606938
881.701466	56076.530588	33.611956
882.532143	56128.751638	33.616973
883.319001	56194.960704	33.621991
883.959181	56254.643237	33.627008
884.741238	56333.688640	33.632026
885.301152	56399.685183	33.637044
886.103372	56475.943776	33.642061
886.535878	56554.313399	33.647079
887.438676	56624.340996	33.652096
888.369838	56719.852021	33.657114
889.170600	56795.884889	33.662132
889.903470	56881.673881	33.667149
890.569790	56975.804671	33.672167
891.767772	57072.234735	33.677184
892.286767	57168.830181	33.682202
893.273752	57257.519502	33.687220
894.337621	57349.985258	33.692237
895.084563	57454.586474	33.697255
895.870117	57548.795924	33.702272
896.584795	57635.077483	33.707290
897.774822	57744.885044	33.712308
898.699844	57838.104597	33.717325
899.743854	57943.463175	33.722343
900.935937	58031.084935	33.727360
901.115186	58132.481281	33.732378
902.284736	58220.959918	33.737396
903.538510	58300.257554	33.742413
904.580190	58418.462018	33.747431
905.448486	58515.681370	33.752448
906.323513	58597.777732	33.757466
907.203043	58692.798897	33.762484
908.483780	58793.609995	33.767501
908.941561	58883.770995	33.772519
909.942642	58986.465093	33.777536
910.971249	59081.388753	33.782554
911.545980	59178.165774	33.787572
912.667364	59275.014169	33.792589
913.526407	59377.707774	33.797607
914.701510	59468.439420	33.802624
915.629217	59557.786959	33.807642
916.481872	59669.576059	33.812660
917.731029	59757.938856	33.817677
918.705820	59858.633924	33.822695
919.351695	59937.113362	33.827712
920.690923	60025.980898	33.832730
921.649392	60110.116607	33.837748
923.090448	60198.327823	33.842765
923.781192	60275.475456	33.847783
924.627670	60368.338168	33.852800
925.545993	60445.494493	33.857818
925.930802	60544.544260	33.862836
927.085773	60631.416942	33.867853
927.733879	60735.575585	33.872871
929.158966	60812.311782	33.877888
930.129365	60899.445573	33.882906
930.966763	60982.691967	33.887924
932.044717	61058.019336	33.892941
932.426490	61135.178629	33.897959
933.404223	61203.838083	33.902976
934.259340	61302.835963	33.907994
934.918754	61382.519173	33.913012
936.001335	61473.714184	33.918029
936.727388	61559.165889	33.923047
937.554610	61650.497117	33.928064
938.493868	61728.779500	33.933082
939.012276	61838.923311	33.938100
940.678381	61917.122399	33.943117
941.307758	62022.011097	33.948135
942.101861	62117.303250	33.953152
942.822250	62214.476968	33.958170
943.822034	62320.798818	33.963188
944.847129	62418.395601	33.968205
945.544960	62518.927980	33.973223
946.603558	62626.862118	33.978240
947.893395	62731.788610	33.983258
948.437405	62832.820800	33.988276
949.963156	62935.080440	33.993293
950.708585	63038.810030	33.998311
951.665901	63133.689769	34.003328
952.706227	63234.840919	34.008346
953.797484	63340.276062	34.013364
954.677017	63441.990742	34.018381
955.560685	63549.171656	34.023399
956.777805	63644.723146	34.028416
957.677354	63749.461585	34.033434
958.296818	63852.852503	34.038452
959.409782	63946.454672	34.043469
960.583337	64044.519383	34.048487
961.472389	64162.121129	34.053504
962.474593	64250.203258	34.058522
963.405582	64369.072296	34.063540
964.437550	64455.890578	34.068557
965.284647	64563.676743	34.073575
966.554327	64661.805133	34.078592
967.748909	64752.180176	34.083610
968.651769	64857.581070	34.088628
969.725155	64960.694180	34.093645
970.640173	65055.100720	34.098663
971.502328	65138.904661	34.103680
973.062372	65235.919184	34.108698
973.798378	65340.572372	34.113716
974.823757	65435.039027	34.118733
975.727531	65528.644346	34.123751
976.724934	65626.647310	34.128768
978.024987	65709.790327	34.133786
978.846608	65815.594731	34.138804
979.912454	65891.391724	34.143821
980.856356	65989.051323	34.148839
981.764960	66076.641956	34.153856
982.715332	66171.307355	34.158874
983.534281	66246.652331	34.163892
984.623831	66327.942821	34.168909
984.999985	66424.374762	34.173927
986.105773	66510.704230	34.178944
987.314450	66596.057557	34.183962
987.789887	66684.632658	34.188980
989.092396	66774.722129	34.193997
990.057474	66859.537386	34.199015
990.738048	66960.086422	34.204032
991.612023	67059.525007	34.209050
992.434815	67156.909742	34.214068
993.543117	67260.516055	34.219085
994.436113	67374.984662	34.224103
995.630783	67471.193692	34.229120
996.291604	67577.033348	34.234138
997.198263	67675.152773	34.239156
998.038568	67778.772914	34.244173
999.290330	67894.071922	34.249191
1000.292878	68001.855784	34.254208
1001.201553	68112.396899	34.259226
1002.407477	68225.601501	34.264244
1003.579259	68335.621909	34.269261
1004.319093	68449.577930	34.274279
1005.123354	68556.657276	34.279296
1006.334383	68670.211118	34.284314
1007.532822	68783.723402	34.289332
1008.676399	68879.151533	34.294349
1009.748793	68988.010056	34.299367
1010.989780	69096.981354	34.304384
1012.097568	69200.389623	34.309402
1013.279718	69310.274902	34.314420
1014.047008	69416.057085	34.319437
1015.039084	69507.797560	34.324455
1016.133780	69631.098569	34.329472
1017.041544	69722.215363	34.334490
1018.104006	69833.272473	34.339508
1019.173282	69936.488592	34.344525
1020.484679	70046.332176	34.349543
1021.291109	70160.167543	34.354560
1022.724108	70256.794690	34.359578
1023.585374	70357.942221	34.364596
1024.682079	70461.649551	34.369613
1025.857150	70569.483331	34.374631
1026.236754	70670.778596	34.379648
1027.434088	70778.856391	34.384666
1028.656825	70891.675724	34.389684
1029.733376	70988.950775	34.394701
1030.763757	71093.840869	34.399719
1031.683722	71198.123572	34.404736
1033.057433	71302.037683	34.409754
1034.270462	71397.549176	34.414772
1035.213974	71489.654153	34.419789
1036.266088	71595.642864	34.424807
1036.918965	71704.608475	34.429824
1038.258158	71784.356118	34.434842
1039.165492	71889.958736	34.439860
1039.947919	71974.913738	34.444877
1040.927429	72072.430720	34.449895
1041.792488	72162.472492	34.454912
1043.164277	72252.800549	34.459930
1043.778595	72346.775340	34.464948
1045.127095	72448.961858	34.469965
1045.981548	72542.153766	34.474983
1046.534315	72649.763013	34.480000
1047.957497	72738.246342	34.485018
1049.140632	72844.081881	34.490036
1049.887292	72961.715258	34.495053
1051.233926	73055.715928	34.500071
1051.787285	73171.112802	34.505088
1053.115838	73264.137896	34.510106
1054.119415	73380.304790	34.515124
1055.082499	73480.036634	34.520141
1056.273984	73599.258608	34.525159
1057.203052	73712.273426	34.530176
1058.690257	73821.876225	34.535194
1059.417272	73936.023983	34.540212
1060.250504	74050.408265	34.545229
1061.486430	74149.303830	34.550247
1062.462900	74273.303473	34.555264
1063.686807	74382.414089	34.560282
1064.454954	74510.859234	34.565300
1065.588353	74623.751908	34.570317
1066.686303	74724.915654	34.575335
1067.473908	74853.549480	34.580352
1069.121869	74968.017946	34.585370
1069.902958	75086.789540	34.590388
1070.925958	75206.471294	34.595405
1072.347346	75319.094563	34.600423
1073.329046	75439.011776	34.605440
1074.710843	75555.466064	34.610458
1075.967788	75670.904447	34.615476
1076.838184	75796.472377	34.620493
1077.906901	75902.557163	34.625511
1078.871603	76008.772808	34.630528
1080.397604	76114.956610	34.635546
1081.396772	76236.297756	34.640564
1082.321605	76353.556125	34.645581
1083.831646	76454.960053	34.650599
1084.745522	76568.467343	34.655616
1085.635931	76677.396964	34.660634
1086.804508	76797.817082	34.665652
1088.078488	76911.104690	34.670669
1088.971397	77015.049151	34.675687
1089.791446	77141.075838	34.680704
1091.209641	77248.369809	34.685722
1091.958462	77362.520854	34.690740
1092.967905	77482.648010	34.695757
1094.342956	77599.778768	34.700775
1095.209961	77713.394714	34.705792
1096.711402	77823.743861	34.710810
1097.604520	77933.646804	34.715828
1098.510867	78029.074356	34.720845
1099.806984	78131.860626	34.725863
1100.623678	78241.467678	34.730880
1101.900819	78342.772703	34.735898
1103.467474	78450.795225	34.740916
1104.270087	78545.331521	34.745933
1105.601879	78653.455675	34.750951
1106.556624	78753.474034	34.755968
1107.582238	78844.961276	34.760986
1108.363930	78961.353564	34.766004
1109.026443	79077.955091	34.771021
1110.646040	79183.116061	34.776039
1111.349123	79299.421634	34.781056
1112.518855	79421.557364	34.786074
1113.666442	79543.286481	34.791092
1114.465839	79660.097092	34.796109
1115.842074	79771.475371	34.801127
1117.080181	79898.185786	34.806144
1118.160195	80020.434155	34.811162
1119.059068	80152.130527	34.816180
1120.113556	80266.748501	34.821197
1121.486944	80383.155860	34.826215
1122.636510	80523.639116	34.831232
1123.997820	80633.058519	34.836250
1124.987544	80757.525412	34.841268
1126.051171	80887.411334	34.846285
1127.629276	80998.321635	34.851303
1128.575648	81134.150887	34.856320
1129.805454	81244.599543	34.861338
1130.721919	81365.838833	34.866356
1131.674405	81486.263946	34.871373
1133.320193	81611.503994	34.876391
1134.365104	81730.935982	34.881408
1135.572212	81853.004270	34.886426
1136.607682	81968.235232	34.891444
1137.623300	82105.526443	34.896461
1139.260439	82216.806846	34.901479
1140.156773	82342.707834	34.906496
1141.283312	82462.744247	34.911514
1142.594003	82583.061835	34.916532
1143.432643	82706.205214	34.921549
1145.187619	82823.810979	34.926567
1146.021426	82938.858101	34.931584
1147.312006	83068.095654	34.936602
1148.754230	83185.095700	34.941620
1149.573697	83305.223713	34.946637
1150.706166	83417.026991	34.951655
1151.886107	83543.427475	34.956672
1153.058502	83660.270774	34.961690
1154.210166	83773.318367	34.966708
1155.259928	83904.831112	34.971725
1156.707562	84002.653134	34.976743
1157.866058	84123.939466	34.981760
1158.785638	84243.260302	34.986778
1160.473908	84342.379655	34.991796
1161.621127	84450.525417	34.996813
1162.582170	84536.111228	35.001831
1163.308458	84654.194314	35.006848
1164.783035	84749.031308	35.011866
1165.972672	84866.510805	35.016884
1166.823726	84961.827263	35.021901
1167.809668	85070.931266	35.026919
1168.660665	85179.949807	35.031936
1169.756640	85316.414619	35.036954
1170.962550	85419.200693	35.041972
1172.246284	85551.179648	35.046989
1173.344029	85661.527138	35.052007
1174.179342	85779.535926	35.057024
1175.393426	85913.266980	35.062042
1177.031980	86038.610446	35.067060
1178.070419	86160.389105	35.072077
1179.468592	86281.637032	35.077095
1180.579586	86396.115122	35.082112
1181.607928	86531.384467	35.087130
1182.746320	86643.937326	35.092148
1183.728246	86776.629468	35.097165
1185.203135	86891.140870	35.102183
1185.978685	87032.454250	35.107200
1187.359446	87167.861277	35.112218
1188.669323	87293.251732	35.117236
1189.864272	87435.797349	35.122253
1191.306082	87559.125952	35.127271
1192.405105	87691.906315	35.132288
1193.458647	87826.237646	35.137306
1195.137655	87962.354749	35.142324
1196.000660	88082.528136	35.147341
1197.679967	88204.026805	35.152359
1198.598973	88343.226580	35.157376
1199.922338	88472.472827	35.162394
1201.255187	88602.205262	35.167412
1202.012070	88742.913127	35.172429
1203.405913	88860.628733	35.177447
1204.774643	88994.164698	35.182464
1205.525955	89132.220000	35.187482
1206.834373	89254.555063	35.192500
1208.081358	89402.607148	35.197517
1209.409139	89525.320093	35.202535
1210.641813	89670.985845	35.207552
1211.663179	89793.110306	35.212570
1213.110757	89919.834819	35.217588
1214.471733	90064.667009	35.222605
1215.926011	90180.672674	35.227623
1216.943481	90312.476557	35.232640
1217.971018	90455.625225	35.237658
1219.612853	90581.804122	35.242676
1220.988883	90715.064915	35.247693
1222.447875	90830.845620	35.252711
1223.000577	90947.884122	35.257728
1224.682174	91079.454227	35.262746
1225.905327	91195.268037	35.267764
1226.487097	91316.515938	35.272781
1227.766979	91416.270485	35.277799
1228.920395	91546.902817	35.282816
1230.151051	91663.160622	35.287834
1231.556097	91786.645597	35.292852
1232.632324	91901.967885	35.297869
1233.729026	92022.144845	35.302887
1234.725103	92147.018719	35.307904
1235.834684	92269.971516	35.312922
1237.429467	92409.058182	35.317940
1238.525996	92540.692122	35.322957
1239.520607	92661.046919	35.327975
1240.691330	92798.400888	35.332992
1241.604884	92935.240008	35.338010
1243.510625	93067.064672	35.343028
1244.589536	93211.873934	35.348045
1246.032688	93347.132379	35.353063
1247.082455	93479.860922	35.358080
1248.609657	93620.148739	35.363098
1249.810821	93757.276112	35.368116
1251.047121	93904.259692	35.373133
1252.316525	94022.750219	35.378151
1254.005874	94151.838974	35.383168
1255.205293	94294.782841	35.388186
1256.411235	94420.439476	35.393204
1257.614687	94561.018738	35.398221
1259.053591	94692.433900	35.403239
1260.123591	94834.876795	35.408256
1261.201025	94966.072716	35.413274
1262.632528	95103.816951	35.418292
1264.106387	95246.678999	35.423309
1265.284819	95378.898674	35.428327
1266.850301	95515.340045	35.433344
1267.980213	95657.411759	35.438362
1269.204139	95781.371574	35.443380
1270.701020	95923.487841	35.448397
1271.673252	96055.269849	35.453415
1272.833481	96191.678544	35.458432
1274.171923	96325.282681	35.463450
1276.013551	96464.083412	35.468468
1276.972591	96614.064072	35.473485
1278.223006	96753.074438	35.478503
1279.657727	96875.728916	35.483520
1280.964563	97016.509543	35.488538
1282.248748	97135.343123	35.493556
1283.365243	97285.594203	35.498573
1284.829714	97423.265150	35.503591
1285.983110	97563.415647	35.508608
1286.969434	97703.726421	35.513626
1288.583561	97830.596133	35.518644
1289.581935	97984.229867	35.523661
1290.715750	98116.384092	35.528679
1292.139415	98263.435954	35.533696
1293.415086	98397.821458	35.538714
1294.645118	98525.907518	35.543732
1295.801815	98655.631867	35.548749
1296.907645	98787.591982	35.553767
1298.631141	98922.782449	35.558784
1299.462160	99059.153158	35.563802
1301.184249	99176.732054	35.568820
1302.367669	99318.647374	35.573837
1303.290839	99454.012492	35.578855
1304.784974	99587.313694	35.583872
1305.485712	99725.031364	35.588890
1307.021150	99850.235548	35.593908
1308.287351	100006.630416	35.598925
1309.684983	100159.411762	35.603943
1311.253513	100295.805436	35.608960
1311.768746	100451.088939	35.613978
1313.438536	100596.199554	35.618996
1315.022166	100748.765425	35.624013
1316.112377	100887.952951	35.629031
1317.771286	101045.924830	35.634048
1318.630718	101198.849220	35.639066
1320.202230	101353.173636	35.644084
1321.696610	101504.360351	35.649101
1322.942761	101662.908229	35.654119
1324.320072	101803.422313	35.659136
1325.519381	101964.921922	35.664154
1327.374281	102112.619500	35.669172
1328.841906	102269.826524	35.674189
1329.949112	102418.106797	35.679207
1331.511467	102565.486750	35.684224
1332.525890	102712.062536	35.689242
1334.058229	102870.320027	35.694260
1335.197565	103024.445792	35.699277
1336.565217	103182.282301	35.704295
1338.403813	103319.043110	35.709312
1339.244357	103477.920887	35.714330
1340.654160	103631.368536	35.719348
1342.047748	103782.181029	35.724365
1343.782451	103932.908628	35.729383
1345.398646	104068.291691	35.734400
1346.270154	104232.934428	35.739418
1347.875294	104377.072679	35.744436
1349.129233	104529.184088	35.749453
1350.474299	104683.110824	35.754471
1352.310606	104826.746792	35.759488
1353.271654	104980.198603	35.764506
1354.549285	105124.349167	35.769524
1356.217266	105274.937726	35.774541
1357.402358	105431.850067	35.779559
1358.897326	105571.697172	35.784576
1359.771061	105725.692929	35.789594
1361.597718	105866.830674	35.794612
1362.559333	106026.965672	35.799629
1364.133182	106166.227836	35.804647
1365.708217	106324.767470	35.809664
1367.021140	106467.635856	35.814682
1368.505541	106595.200472	35.819700
1369.519494	106728.732548	35.824717
1370.977742	106862.542832	35.829735
1372.520492	106996.473336	35.834752
1373.402035	107138.173848	35.839770
1374.903827	107273.549045	35.844788
1376.514058	107410.540617	35.849805
1377.385145	107551.416145	35.854823
1379.082459	107671.649095	35.859840
1379.839311	107832.119819	35.864858
1381.284696	107971.368583	35.869876
1382.981574	108126.388148	35.874893
1384.118773	108271.459721	35.879911
1385.854202	108427.557367	35.884928
1386.935157	108574.316915	35.889946
1388.457409	108723.513582	35.894964
1389.721919	108881.296616	35.899981
1391.197143	109036.180017	35.904999
1392.714005	109188.051358	35.910016
1394.080698	109347.087042	35.915034
1395.191572	109490.106710	35.920052
1396.941296	109650.165828	35.925069
1398.208358	109809.169728	35.930087
1399.903622	109965.131730	35.935104
1401.029062	110128.882048	35.940122
1402.696150	110285.496190	35.945140
1403.696935	110431.368202	35.950157
1405.100974	110600.875361	35.955175
1406.492851	110757.257749	35.960192
1407.951938	110926.992611	35.965210
1409.494899	111091.645129	35.970228
1410.981190	111254.889866	35.975245
1412.394335	111420.634962	35.980263
1413.923613	111578.861729	35.985280
1415.153109	111747.379073	35.990298
1416.316154	111900.190661	35.995316
1418.328658	112064.414243	36.000333
1419.499794	112241.546794	36.005351
1421.009928	112399.193152	36.010368
1422.747568	112568.211373	36.015386
1423.907528	112733.859907	36.020404
1425.520948	112888.663343	36.025421
1426.708555	113045.282579	36.030439
1428.845365	113209.050862	36.035456
1430.316939	113375.755629	36.040474
1431.856503	113519.357251	36.045492
1433.286481	113679.784533	36.050509
1434.552309	113840.618762	36.055527
1436.199726	113991.808916	36.060544
1437.563997	114149.685775	36.065562
1438.857340	114293.672822	36.070580
1440.431677	114449.156858	36.075597
1441.926598	114613.523808	36.080615
1443.150904	114767.425781	36.085632
1444.671168	114921.933736	36.090650
1446.477893	115059.246902	36.095668
1447.486911	115203.113403	36.100685
1449.108344	115340.052368	36.105703
1450.555918	115466.073524	36.110720
1451.480589	115614.539364	36.115738
1452.861317	115756.412672	36.120756
1453.987766	115906.386591	36.125773
1455.449622	116049.875727	36.130791
1456.964827	116193.699077	36.135808
1458.462167	116354.088364	36.140826
1459.602379	116511.160888	36.145844
1461.231737	116675.975722	36.150861
1462.584470	116831.940144	36.155879
1463.950925	116985.098571	36.160896
1465.186437	117163.243226	36.165914
1466.465589	117329.175262	36.170932
1468.087223	117495.300878	36.175949
1469.450362	117675.258600	36.180967
1471.071425	117837.973863	36.185984
1472.354506	118014.154104	36.191002
1473.730787	118187.902070	36.196020
1475.306924	118367.976425	36.201037
1476.738178	118554.501727	36.206055
1478.494543	118717.409999	36.211072
1480.388575	118898.501278	36.216090
1481.678246	119073.522663	36.221108
1483.545330	119242.241927	36.226125
1485.184030	119421.262595	36.231143
1486.661482	119579.478019	36.236160
1487.971994	119756.476269	36.241178
1489.307533	119933.370434	36.246196
1491.422645	120108.103007	36.251213
1492.535467	120288.568268	36.256231
1494.271111	120453.472689	36.261248
1495.580468	120622.435168	36.266266
1497.158504	120803.779899	36.271284
1498.883521	120960.723254	36.276301
1500.022564	121142.456695	36.281319
1501.513414	121320.918655	36.286336
1503.564684	121489.844836	36.291354
1505.328187	121649.952402	36.296372
1507.188369	121817.897862	36.301389
1508.215834	121990.358806	36.306407
1509.881111	122147.584708	36.311424
1511.605005	122313.313251	36.316442
1513.057384	122477.160850	36.321460
1514.534366	122644.653178	36.326477
1516.594416	122806.797769	36.331495
1517.625200	122952.046435	36.336512
1518.642572	123136.219378	36.341530
1520.298929	123292.921544	36.346548
1521.971474	123468.506697	36.351565
1523.316246	123638.800099	36.356583
1524.804433	123798.799746	36.361600
1526.272184	123968.721070	36.366618
1527.587006	124123.113837	36.371636
1529.346724	124267.785218	36.376653
1530.614738	124419.400583	36.381671
1532.090493	124574.821682	36.386688
1533.716876	124734.450313	36.391706
1534.900603	124897.329493	36.396724
1536.475001	125048.393076	36.401741
1537.592705	125222.101903	36.406759
1539.151125	125371.396515	36.411776
1540.486143	125552.419604	36.416794
1541.839268	125732.681018	36.421812
1543.840368	125907.976600	36.426829
1545.189408	126075.270039	36.431847
1546.941430	126254.914212	36.436864
1548.531673	126442.324903	36.441882
1549.691502	126613.743210	36.446900
1551.364278	126788.349273	36.451917
1552.877653	126973.926410	36.456935
1554.743763	127155.053155	36.461952
1556.199275	127337.867780	36.466970
1557.710476	127517.533202	36.471988
1559.534155	127707.271683	36.477005
1560.842059	127888.808657	36.482023
1562.561221	128068.989373	36.487040
1564.310418	128257.628716	36.492058
1566.016092	128436.002457	36.497076
1568.328058	128600.852799	36.502093
1569.722283	128772.627419	36.507111
1571.515364	128940.184543	36.512128
1573.335721	129115.428058	36.517146
1574.707075	129290.325951	36.522164
1576.258095	129455.264270	36.527181
1577.804416	129637.889707	36.532199
1579.370912	129806.096157	36.537216
1581.125544	129984.383423	36.542234
1582.596513	130164.718572	36.547252
1584.255984	130337.841652	36.552269
1585.575823	130507.282398	36.557287
1587.301879	130683.120881	36.562304
1589.068813	130864.021647	36.567322
1590.577558	131034.385765	36.572340
1592.145370	131205.805758	36.577357
1593.601920	131393.309287	36.582375
1595.546041	131568.776611	36.587392
1596.877020	131751.285351	36.592410
1598.183727	131920.990106	36.597428
1600.209754	132100.818763	36.602445
1601.726553	132278.410878	36.607463
1603.338754	132464.021666	36.612480
1605.289969	132623.390986	36.617498
1606.606920	132793.834206	36.622516
1608.097717	132981.178118	36.627533
1609.720197	133158.784298	36.632551
1611.614834	133335.816204	36.637568
1612.969719	133503.457516	36.642586
1614.356713	133672.703856	36.647604
1616.309954	133826.783357	36.652621
1617.415215	134001.258627	36.657639
1618.805281	134159.103839	36.662656
1620.329260	134328.028199	36.667674
1621.661313	134498.783292	36.672692
1622.837160	134667.473515	36.677709
1624.753237	134845.195575	36.682727
1626.237656	135023.937621	36.687744
1627.684239	135222.821177	36.692762
1629.056535	135410.250466	36.697780
1630.776192	135604.772397	36.702797
1632.516809	135789.902824	36.707815
1633.978246	135986.863219	36.712832
1636.005344	136177.741469	36.717850
1637.548117	136362.552165	36.722868
1638.945840	136568.067279	36.727885
1641.025808	136767.659128	36.732903
1642.851624	136950.451794	36.737920
1644.694069	137133.521744	36.742938
1646.076053	137353.085389	36.747956
1647.876214	137525.862139	36.752973
1650.039773	137731.149729	36.757991
1651.317269	137923.032806	36.763008
1653.209695	138109.345003	36.768026
1654.604272	138307.497477	36.773044
1656.832184	138494.861328	36.778061
1658.029289	138695.138729	36.783079
1660.013403	138879.781107	36.788096
1662.081738	139080.784484	36.793114
1663.404604	139266.776220	36.798132
1665.213074	139452.159732	36.803149
1666.837110	139631.655390	36.808167
1668.486759	139834.415860	36.813184
1670.398899	140027.859248	36.818202
1672.056372	140220.697995	36.823220
1673.967593	140419.961089	36.828237
1675.561573	140610.429837	36.833255
1677.595647	140791.768342	36.838272
1679.127144	140975.228203	36.843290
1680.572659	141170.489337	36.848308
1682.353606	141344.596689	36.853325
1684.307286	141535.609822	36.858343
1685.851283	141735.624319	36.863360
1687.486501	141912.863188	36.868378
1688.833696	142102.125806	36.873396
1690.908469	142285.418610	36.878413
1692.847662	142475.628817	36.883431
1694.569864	142671.996350	36.888448
1696.606662	142843.473436	36.893466
1697.968940	143035.477113	36.898484
1699.654717	143215.782742	36.903501
1701.482158	143401.149443	36.908519
1702.971451	143590.056496	36.913536
1704.768363	143756.595645	36.918554
1706.391405	143927.840308	36.923572
1708.270285	144086.928119	36.928589
1709.746852	144256.144538	36.933607
1711.092721	144432.277842	36.938624
1712.881935	144590.799437	36.943642
1714.316341	144771.230134	36.948660
1715.703420	144937.752006	36.953677
1717.349237	145115.045701	36.958695
1718.589813	145311.202322	36.963712
1720.623534	145494.761591	36.968730
1722.138018	145679.367733	36.973748
1723.925064	145869.344161	36.978765
1725.715014	146069.233657	36.983783
1727.017851	146266.768034	36.988800
1729.024836	146465.598856	36.993818
1730.600806	146670.786631	36.998836
1732.360938	146863.866275	37.003853
1734.271970	147060.485115	37.008871
1735.615046	147277.882851	37.013888
1737.386120	147484.908331	37.018906
1739.212380	147689.048874	37.023924
1741.239585	147902.856273	37.028941
1742.684801	148115.210990	37.033959
1744.161474	148330.832684	37.038976
1746.080873	148523.745020	37.043994
1747.870137	148753.099455	37.049012
1749.986922	148966.722284	37.054029
1751.722605	149175.539115	37.059047
1753.925211	149390.215998	37.064064
1755.604977	149601.896800	37.069082
1757.297167	149814.654579	37.074100
1759.417883	150020.081655	37.079117
1761.220692	150227.969206	37.084135
1762.663349	150432.771278	37.089152
1764.901959	150635.407188	37.094170
1766.356932	150848.932038	37.099188
1768.465854	151060.047122	37.104205
1770.474895	151262.368412	37.109223
1772.005659	151471.676298	37.114240
1773.868674	151676.787099	37.119258
1775.862853	151881.269816	37.124276
1777.894182	152087.256596	37.129293
1779.523853	152286.551000	37.134311
1780.985464	152490.285304	37.139328
1783.158887	152687.872992	37.144346
1785.143709	152894.962535	37.149364
1787.160608	153095.100500	37.154381
1789.184474	153294.046789	37.159399
1790.883853	153487.923640	37.164416
1792.456402	153677.156013	37.169434
1793.955204	153877.558448	37.174452
1795.510754	154088.260946	37.179469
1797.769466	154279.340330	37.184487
1799.035304	154490.027957	37.189504
1800.950510	154680.644329	37.194522
1802.926464	154864.963303	37.199540
1804.463006	155054.335965	37.204557
1806.373480	155223.680521	37.209575
1807.874759	155414.379442	37.214592
1809.712244	155601.234929	37.219610
1811.167507	155794.644005	37.224628
1813.062745	155969.839944	37.229645
1815.020527	156163.348856	37.234663
1816.603261	156363.702028	37.239680
1818.583981	156551.731894	37.244698
1820.446802	156749.506921	37.249716
1821.853457	156957.753011	37.254733
1823.794029	157150.217821	37.259751
1825.429751	157361.764827	37.264768
1827.359248	157562.399645	37.269786
1829.209211	157758.737000	37.274804
1831.036303	157979.209623	37.279821
1833.255590	158182.540981	37.284839
1834.588427	158396.640439	37.289856
1836.910732	158606.107930	37.294874
1838.614461	158814.267340	37.299892
1840.072331	159026.613592	37.304909
1842.135325	159235.289113	37.309927
1843.822372	159447.715672	37.314944
1845.616084	159668.153576	37.319962
1847.425203	159889.516130	37.324980
1849.351163	160114.044469	37.329997
1851.486050	160340.760268	37.335015
1853.255602	160563.185871	37.340032
1855.059508	160782.056663	37.345050
1857.163484	160998.598532	37.350068
1859.038188	161231.435708	37.355085
1861.189667	161446.311501	37.360103
1862.534744	161675.266341	37.365120
1864.478084	161891.839146	37.370138
1866.395607	162112.779880	37.375156
1868.374492	162340.205329	37.380173
1870.654212	162562.334159	37.385191
1872.827038	162781.830795	37.390208
1874.576088	163007.204418	37.395226
1876.825165	163233.058091	37.400244
1878.304203	163442.611938	37.405261
1880.519272	163649.260063	37.410279
1882.222625	163869.471934	37.415296
1884.231674	164070.219811	37.420314
1886.362249	164290.087399	37.425332
1887.894118	164507.387999	37.430349
1890.186918	164715.830761	37.435367
1891.689117	164935.903429	37.440384
1893.948391	165152.369477	37.445402
1895.881628	165373.809504	37.450420
1897.863132	165578.717315	37.455437
1899.788016	165776.862519	37.460455
1901.615330	165998.589445	37.465472
1903.703279	166193.996816	37.470490
1905.647531	166382.198585	37.475508
1907.303961	166573.351463	37.480525
1909.137158	166748.420144	37.485543
1910.769839	166940.200153	37.490560
1912.551872	167126.364028	37.495578
1914.309181	167318.950621	37.500596
1915.932468	167520.717036	37.505613
1918.069162	167713.486425	37.510631
1919.643481	167917.418961	37.515648
1921.469313	168116.974817	37.520666
1923.439567	168343.893295	37.525684
1925.331502	168550.290239	37.530701
1927.636156	168757.967307	37.535719
1929.374064	168976.542303	37.540736
1930.855670	169185.658790	37.545754
1933.163012	169399.985430	37.550772
1935.016270	169609.882410	37.555789
1937.176262	169825.033925	37.560807
1938.966598	170050.786084	37.565824
1941.284863	170269.923252	37.570842
1943.242835	170479.250235	37.575860
1944.659034	170703.797129	37.580877
1946.835134	170925.878047	37.585895
1948.770624	171150.129467	37.590912
1950.509638	171390.485104	37.595930
1952.868110	171601.872948	37.600948
1954.871396	171827.373310	37.605965
1956.766144	172045.154285	37.610983
1958.800205	172278.834243	37.616000
1960.772485	172499.231258	37.621018
1962.941324	172733.983456	37.626036
1964.629546	172953.984101	37.631053
1967.207751	173164.876112	37.636071
1968.853306	173398.002750	37.641088
1970.999306	173628.400044	37.646106
1973.411402	173842.442667	37.651124
1975.130850	174071.933413	37.656141
1977.272050	174283.027548	37.661159
1979.379048	174516.772512	37.666176
1981.488688	174729.155272	37.671194
1983.434521	174949.126011	37.676212
1985.457028	175181.695751	37.681229
1987.985934	175380.859930	37.686247
1990.246849	175615.500228	37.691264
1991.773009	175822.285196	37.696282
1994.024796	176042.251365	37.701300
1995.877440	176258.184342	37.706317
1997.950160	176462.247040	37.711335
2000.148704	176679.713160	37.716352
2001.811586	176885.390753	37.721370
2003.929190	177085.656125	37.726388
2005.836889	177297.386530	37.731405
2008.404779	177508.378920	37.736423
2009.921949	177714.819594	37.741440
2012.120960	177916.344752	37.746458
2014.614812	178099.757827	37.751476
2016.347846	178280.298292	37.756493
2018.147569	178440.694536	37.761511
2019.954132	178629.953562	37.766528
2021.665073	178825.419971	37.771546
2023.784442	179001.740839	37.776564
2025.608366	179200.895744	37.781581
2027.274421	179384.864474	37.786599
2029.357193	179575.720594	37.791616
2031.467445	179774.756646	37.796634
2033.782400	179976.603163	37.801652
2035.474539	180179.691344	37.806669
2037.573444	180378.655896	37.811687
2039.363739	180592.362735	37.816704
2041.608044	180795.087099	37.821722
2043.790489	180998.900705	37.826740
2045.779951	181200.893461	37.831757
2047.971665	181413.792107	37.836775
2049.868169	181614.253614	37.841792
2051.765077	181845.256233	37.846810
2054.025058	182041.982499	37.851828
2056.290522	182264.059848	37.856845
2058.338130	182470.959640	37.861863
2060.357945	182679.577747	37.866880
2062.661382	182889.090790	37.871898
2064.774598	183098.165542	37.876916
2066.803085	183318.065353	37.881933
2068.976361	183528.338028	37.886951
2071.376343	183741.151531	37.891968
2073.240969	183954.977269	37.896986
2075.514212	184158.943479	37.902004
2077.648847	184370.114490	37.907021
2079.748834	184574.097399	37.912039
2081.827610	184790.354814	37.917056
2084.047927	184990.729560	37.922074
2086.504502	185209.086187	37.927092
2088.119648	185410.421670	37.932109
2090.571874	185603.123503	37.937127
2092.560440	185820.656407	37.942144
2094.844522	186031.126293	37.947162
2097.122838	186221.764615	37.952180
2099.309340	186442.657152	37.957197
2101.418386	186630.963810	37.962215
2103.443471	186854.421837	37.967232
2105.500738	187047.839612	37.972250
2107.791946	187242.883431	37.977268
2109.759625	187450.148808	37.982285
2111.891033	187645.917615	37.987303
2114.146312	187861.958584	37.992320
2115.873652	188058.173927	37.997338
2118.134618	188261.348344	38.002356
2120.389760	188473.407545	38.007373
2122.426653	188670.718459	38.012391
2124.571836	188887.644569	38.017408
2126.276069	189092.941327	38.022426
2128.598307	189273.280877	38.027444
2130.451921	189462.121768	38.032461
2132.513962	189635.270547	38.037479
2134.934415	189817.627042	38.042496
2136.761959	190003.771191	38.047514
2138.835791	190189.090193	38.052532
2140.604592	190375.917708	38.057549
2142.848170	190574.345923	38.062567
2144.749742	190774.263248	38.067584
2146.886336	190959.321469	38.072602
2149.123206	191150.646383	38.077620
2151.203042	191360.170092	38.082637
2153.467160	191560.134697	38.087655
2155.489491	191776.573118	38.092672
2157.562790	191980.592722	38.097690
2159.919139	192186.687672	38.102708
2161.477718	192406.045222	38.107725
2163.888786	192610.293084	38.112743
2165.949613	192825.321341	38.117760
2168.023625	193048.445411	38.122778
2170.427013	193272.609692	38.127796
2172.647243	193493.504308	38.132813
2174.819779	193715.105495	38.137831
2177.461530	193930.160636	38.142848
2179.457084	194166.577381	38.147866
2181.550932	194377.418949	38.152884
2183.942072	194603.710649	38.157901
2186.357813	194830.164457	38.162919
2188.504287	195052.994096	38.167936
2190.713201	195277.185520	38.172954
2193.258727	195489.051588	38.177972
2195.232365	195713.586858	38.182989
2197.544006	195929.299408	38.188007
2199.986680	196155.196414	38.193024
2201.889808	196373.361713	38.198042
2204.182235	196596.568402	38.203060
2206.268411	196824.009859	38.208077
2208.948314	197030.822223	38.213095
2211.313887	197265.481228	38.218112
2213.376927	197485.174307	38.223130
2216.097231	197702.009836	38.228148
2218.110068	197931.853929	38.233165
2219.963609	198142.089090	38.238183
2222.662014	198352.444950	38.243200
2224.324049	198575.100079	38.248218
2226.454706	198799.814179	38.253236
2228.776087	199018.444592	38.258253
2231.372647	199242.591665	38.263271
2233.218139	199469.054638	38.268288
2235.275321	199705.639242	38.273306
2237.689560	199920.260386	38.278324
2240.109555	200138.689346	38.283341
2242.181558	200374.170253	38.288359
2244.616120	200596.825512	38.293376
2246.697434	200808.964378	38.298394
2249.079479	201017.857715	38.303412
2250.855538	201210.968807	38.308429
2253.395945	201405.596790	38.313447
2255.445201	201603.590904	38.318464
2257.423328	201823.416787	38.323482
2259.651528	202017.080981	38.328500
2261.911928	202228.067224	38.333517
2263.866140	202450.628468	38.338535
2266.159823	202662.398075	38.343552
2268.046461	202888.360942	38.348570
2270.165718	203113.386588	38.353588
2272.696601	203341.089687	38.358605
2274.734148	203571.004477	38.363623
2277.035313	203786.064799	38.368640
2278.671425	204040.366365	38.373658
2281.216148	204272.285354	38.378676
2283.706729	204505.292852	38.383693
2285.674811	204763.442020	38.388711
2288.215857	205006.129040	38.393728
2290.147186	205252.760063	38.398746
2292.840194	205500.312276	38.403764
2295.117145	205763.151834	38.408781
2297.462515	206007.156178	38.413799
2300.016499	206258.643476	38.418816
2302.182261	206514.369846	38.423834
2304.768356	206760.357547	38.428852
2307.330700	207002.516314	38.433869
2309.151747	207268.951237	38.438887
2311.948318	207516.660537	38.443904
2314.275308	207765.295857	38.448922
2316.737318	208011.397255	38.453940
2318.885275	208280.196816	38.458957
2321.214792	208529.558483	38.463975
2323.787036	208772.801870	38.468992
2326.102723	209037.020743	38.474010
2328.569811	209287.620488	38.479028
2331.266064	209533.348134	38.484045
2333.226785	209786.327982	38.489063
2336.048871	210042.307977	38.494080
2338.255414	210288.306688	38.499098
2340.253442	210541.664545	38.504116
2342.775917	210799.789853	38.509133
2345.203496	211047.140277	38.514151
2347.335529	211306.510223	38.519168
2349.587028	211574.482452	38.524186
2352.087674	211819.196358	38.529204
2354.746721	212084.008427	38.534221
2356.700652	212340.973278	38.539239
2359.267396	212586.771447	38.544256
2361.552717	212851.836354	38.549274
2364.077793	213105.412824	38.554292
2366.227339	213376.773060	38.559309
2368.242087	213631.041868	38.564327
2371.024654	213888.820939	38.569344
2373.050530	214141.312531	38.574362
2375.004462	214386.859118	38.579380
2377.490728	214630.417820	38.584397
2379.625097	214865.247549	38.589415
2382.156783	215102.490844	38.594432
2384.133208	215355.959758	38.599450
2386.537447	215596.208578	38.604468
2388.816477	215853.465617	38.609485
2391.011168	216112.577951	38.614503
2393.466519	216362.280073	38.619520
2395.619762	216629.424987	38.624538
2398.026605	216886.640237	38.629556
2400.490005	217156.163022	38.634573
2402.447987	217439.885469	38.639591
2405.162011	217710.945026	38.644608
2407.545419	217977.741194	38.649626
2409.982735	218252.757244	38.654644
2412.285251	218539.324320	38.659661
2414.854352	218820.670013	38.664679
2417.609132	219090.268238	38.669696
2420.094652	219380.504422	38.674714
2422.406255	219669.804370	38.679732
2424.888943	219941.391511	38.684749
2427.112026	220226.441520	38.689767
2429.759474	220511.196816	38.694784
2432.394113	220797.974074	38.699802
2434.918882	221081.595568	38.704820
2437.362083	221363.466158	38.709837
2439.708722	221658.190005	38.714855
2442.489101	221939.729962	38.719872
2445.081244	222232.017337	38.724890
2447.299169	222541.024098	38.729908
2449.734639	222858.060480	38.734925
2452.149491	223152.118996	38.739943
2454.865448	223434.957079	38.744960
2457.352679	223735.570938	38.749978
2459.399270	224023.062963	38.754996
2462.279395	224320.747114	38.760013
2464.502216	224619.057166	38.765031
2467.422835	224904.864719	38.770048
2469.870113	225203.979418	38.775066
2472.558588	225494.079614	38.780084
2475.387277	225779.650868	38.785101
2477.627704	226065.367145	38.790119
2480.154183	226352.131100	38.795136
2482.494889	226641.452396	38.800154
2485.031699	226933.308623	38.805172
2487.908034	227215.766246	38.810189
2490.065397	227513.449563	38.815207
2492.714474	227793.354707	38.820224
2495.003214	228088.733536	38.825242
2497.342652	228381.641877	38.830260
2500.292373	228666.937082	38.835277
2502.720542	228969.128515	38.840295
2505.177768	229247.341790	38.845312
2507.724910	229524.855978	38.850330
2509.980551	229782.150451	38.855348
2512.557335	230049.858352	38.860365
2514.835928	230315.582540	38.865383
2517.206778	230570.194318	38.870400
2519.631538	230832.468240	38.875418
2521.919912	231106.040944	38.880436
2524.504199	231377.104020	38.885453
2526.562707	231657.572090	38.890471
2528.928365	231927.249162	38.895488
2531.132640	232216.737343	38.900506
2533.453217	232505.522243	38.905524
2536.330092	232793.178555	38.910541
2538.796869	233097.866499	38.915559
2541.587164	233388.255891	38.920576
2544.107174	233687.375109	38.925594
2546.408604	234001.159189	38.930612
2549.204383	234299.728616	38.935629
2551.290507	234606.411849	38.940647
2553.697582	234916.448542	38.945664
2556.747348	235233.851483	38.950682
2559.316901	235542.670628	38.955700
2561.994765	235856.705649	38.960717
2564.247640	236180.231870	38.965735
2567.183388	236486.532149	38.970752
2569.703960	236806.182687	38.975770
2572.214496	237119.257474	38.980788
2575.186744	237441.733831	38.985805
2577.577446	237759.782280	38.990823
2580.141978	238080.598021	38.995840
2582.496584	238411.633038	39.000858
2585.282102	238741.940392	39.005876
2588.232159	239056.652868	39.010893
2590.564490	239387.313333	39.015911
2593.367998	239714.369580	39.020928
2595.956549	240033.637764	39.025946
2598.998911	240371.910041	39.030964
2601.546216	240687.630619	39.035981
2603.810584	241014.191773	39.040999
2606.331492	241345.691545	39.046016
2609.338522	241665.405862	39.051034
2612.037993	241992.662746	39.056052
2615.029072	242315.505502	39.061069
2617.439668	242648.296314	39.066087
2620.087097	242966.572399	39.071104
2623.007994	243282.951749	39.076122
2625.343286	243615.731654	39.081140
2628.379971	243940.552589	39.086157
2630.831843	244256.805452	39.091175
2633.780573	244572.624755	39.096192
2636.301749	244895.878708	39.101210
2638.917022	245215.359246	39.106228
2641.831306	245531.160876	39.111245
2644.441863	245848.586202	39.116263
2646.842984	246165.969237	39.121280
2649.623476	246476.663275	39.126298
2652.036676	246776.519209	39.131316
2654.775042	247052.472784	39.136333
2656.957341	247348.607160	39.141351
2659.403042	247636.927695	39.146368
2661.755374	247939.920015	39.151386
2663.976981	248244.178319	39.156404
2666.733135	248546.066451	39.161421
2669.133939	248861.448734	39.166439
2671.555085	249181.705491	39.171456
2674.237803	249497.603242	39.176474
2676.241913	249831.720325	39.181492
2679.073005	250162.354111	39.186509
2682.024275	250511.639642	39.191527
2684.549096	250841.459676	39.196544
2687.274760	251188.343832	39.201562
2689.723756	251535.069317	39.206580
2692.513847	251872.647661	39.211597
2695.055250	252237.674557	39.216615
2697.566027	252582.919049	39.221632
2700.561090	252944.649508	39.226650
2703.355091	253313.550476	39.231668
2706.168689	253670.357743	39.236685
2708.552177	254036.251533	39.241703
2711.314972	254407.064746	39.246720
2714.558519	254769.800852	39.251738
2717.181771	255140.916982	39.256756
2720.476316	255501.639575	39.261773
2722.961376	255870.365720	39.266791
2725.539428	256232.701812	39.271808
2729.132883	256593.556767	39.276826
2731.519836	256960.496777	39.281844
2734.527319	257324.011393	39.286861
2737.539341	257691.387050	39.291879
2740.070740	258046.697028	39.296896
2743.079484	258406.733017	39.301914
2745.851527	258778.441413	39.306932
2748.592828	259133.033886	39.311949
2751.202922	259490.772168	39.316967
2754.207746	259854.646684	39.321984
2756.963994	260213.759963	39.327002
2759.714712	260586.973122	39.332020
2762.631603	260959.296775	39.337037
2765.335794	261314.380696	39.342055
2768.296891	261679.966543	39.347072
2771.235644	262042.609648	39.352090
2773.919733	262406.538259	39.357108
2776.592583	262763.813505	39.362125
2779.667749	263127.731812	39.367143
2782.373566	263490.286446	39.372160
2785.173991	263846.577341	39.377178
2787.779876	264213.721099	39.382196
2790.319180	264576.735073	39.387213
2793.378346	264943.502933	39.392231
2795.971511	265306.407456	39.397248
2798.896132	265654.526000	39.402266
2801.325947	265999.217560	39.407284
2803.911958	266341.928614	39.412301
2806.360371	266674.856090	39.417319
2809.040024	267016.612902	39.422336
2811.646632	267362.141199	39.427354
2814.377262	267718.802115	39.432372
2817.386591	268064.978398	39.437389
2820.018203	268420.436100	39.442407
2822.355721	268767.938556	39.447424
2825.150577	269142.143865	39.452442
2828.115321	269510.581338	39.457460
2831.070929	269874.193822	39.462477
2833.730111	270252.765187	39.467495
2836.369244	270631.136681	39.472512
2839.277197	271006.544388	39.477530
2841.943285	271398.070881	39.482548
2844.406887	271779.823884	39.487565
2847.659400	272172.909022	39.492583
2850.755691	272565.002885	39.497600
2853.586280	272966.131733	39.502618
2855.924224	273364.010839	39.507636
2859.067976	273770.247169	39.512653
2861.931232	274174.114656	39.517671
2864.875476	274588.689611	39.522688
2867.986992	274986.522664	39.527706
2870.888919	275399.707183	39.532724
2873.836991	275798.785498	39.537741
2876.738710	276208.108715	39.542759
2879.797390	276615.705019	39.547776
2882.632861	277027.960035	39.552794
2885.602628	277444.664721	39.557812
2888.403997	277848.694282	39.562829
2891.602587	278267.598049	39.567847
2894.327797	278685.179457	39.572864
2897.555509	279093.993209	39.577882
2900.305278	279508.369610	39.582900
2903.209350	279924.448836	39.587917
2906.075059	280345.538403	39.592935
2908.779847	280771.378251	39.597952
2912.797125	281175.315634	39.602970
2915.396991	281605.693399	39.607988
2918.210882	282016.806714	39.613005
2921.331209	282426.448658	39.618023
2924.167252	282848.659120	39.623040
2927.334474	283253.847471	39.628058
2930.546268	283664.261512	39.633076
2933.474936	284085.465581	39.638093
2936.399912	284496.711818	39.643111
2939.267304	284909.516387	39.648128
2942.382150	285313.847552	39.653146
2945.122286	285725.528325	39.658164
2948.065288	286137.430584	39.663181
2951.241867	286548.761957	39.668199
2954.050911	286967.187683	39.673216
2957.221028	287354.716547	39.678234
2959.870432	287743.394327	39.683252
2962.555353	288113.420290	39.688269
2965.028546	288478.627393	39.693287
2968.186957	288876.165040	39.698304
2971.042275	289250.735192	39.703322
2973.825574	289635.553592	39.708340
2976.803741	290020.874085	39.713357
2979.764713	290407.924154	39.718375
2982.425982	290803.149970	39.723392
2985.369736	291190.176234	39.728410
2988.231864	291603.252503	39.733428
2991.057916	292007.188884	39.738445
2994.255214	292423.843301	39.743463
2996.937675	292840.680097	39.748480
3000.253687	293254.367576	39.753498
3003.235555	293680.757580	39.758516
3005.720082	294099.553989	39.763533
3008.920737	294526.720601	39.768551
3011.701797	294962.564126	39.773568
3015.203324	295383.356229	39.778586
3018.244550	295818.724930	39.783604
3021.331491	296246.972869	39.788621
3024.483040	296685.853086	39.793639
3027.488428	297128.235497	39.798656
3030.900369	297552.567985	39.803674
3033.824525	297992.929046	39.808692
3037.013103	298437.590883	39.813709
3040.675110	298861.321880	39.818727
3043.269217	299309.504825	39.823744
3046.453383	299744.917822	39.828762
3049.569054	300190.221712	39.833780
3052.510421	300625.848637	39.838797
3055.647304	301068.073201	39.843815
3058.700164	301516.126726	39.848832
3062.242113	301946.574724	39.853850
3065.027377	302391.010295	39.858868
3067.892147	302844.830371	39.863885
3071.330236	303271.303065	39.868903
3074.079916	303734.232173	39.873920
3077.384723	304168.572205	39.878938
3080.585031	304624.086273	39.883956
3083.683349	305067.498876	39.888973
3086.354816	305522.712670	39.893991
3089.580045	305979.056523	39.899008
3092.888690	306428.883108	39.904026
3095.976798	306886.972760	39.909044
3098.814048	307342.814469	39.914061
3102.225096	307788.327490	39.919079
3105.260981	308253.786544	39.924096
3108.179275	308700.644294	39.929114
3111.060145	309161.044462	39.934132
3114.294088	309620.193214	39.939149
3117.648535	310084.375663	39.944167
3120.491325	310545.741693	39.949184
3123.766126	310991.010468	39.954202
3126.779879	311423.695334	39.959220
3129.574562	311847.269475	39.964237
3132.529650	312273.102556	39.969255
3135.320099	312703.912869	39.974272
3138.621685	313128.621048	39.979290
3141.445236	313572.198365	39.984308
3144.261207	314011.050870	39.989325
3147.796375	314447.222488	39.994343
3150.363712	314900.486257	39.999360
3153.181326	315347.815997	40.004378
3156.441273	315809.347647	40.009396
3159.780918	316282.598547	40.014413
3162.884821	316755.630520	40.019431
3166.070711	317214.957751	40.024448
3169.252379	317686.449052	40.029466
3172.385301	318162.288769	40.034484
3175.501925	318644.122521	40.039501
3179.127044	319110.304717	40.044519
3182.052473	319599.148112	40.049536
3185.155419	320080.113099	40.054554
3188.394455	320571.441416	40.059572
3191.456749	321069.068058	40.064589
3194.817163	321566.213015	40.069607
3198.406756	322052.550745	40.074624
3201.121048	322557.055754	40.079642
3204.385793	323053.978813	40.084660
3207.467286	323563.270524	40.089677
3211.163803	324071.369841	40.094695
3214.376718	324578.196603	40.099712
3217.920611	325085.044092	40.104730
3221.009054	325586.195710	40.109748
3224.084312	326099.282162	40.114765
3227.460582	326605.105472	40.119783
3231.018121	327127.606852	40.124800
3234.071677	327634.414259	40.129818
3237.855957	328148.162516	40.134836
3240.742806	328654.253192	40.139853
3244.539347	329166.672188	40.144871
3247.657844	329686.051424	40.149888
3250.728654	330188.674535	40.154906
3254.021789	330694.128590	40.159924
3257.391557	331209.140484	40.164941
3261.016204	331714.103379	40.169959
3263.954228	332237.632328	40.174976
3267.230126	332742.109924	40.179994
3270.952047	333252.658488	40.185012
3274.288564	333770.399692	40.190029
3277.564643	334267.477033	40.195047
3280.765778	334779.671154	40.200064
3284.107023	335290.645856	40.205082
3287.718282	335800.101273	40.210100
3290.770440	336310.504601	40.215117
3294.063689	336807.332147	40.220135
3297.331545	337318.277647	40.225152
3300.742863	337811.651121	40.230170
3303.871322	338286.047683	40.235188
3306.857307	338757.289444	40.240205
3310.311920	339216.850073	40.245223
3313.033016	339694.068270	40.250240
3316.238967	340170.825333	40.255258
3319.480003	340642.901447	40.260276
3322.573306	341124.797880	40.265293
3325.678284	341610.471794	40.270311
3328.373373	342103.112660	40.275328
3331.459444	342601.324150	40.280346
3335.011888	343107.734643	40.285364
3338.103809	343635.641946	40.290381
3341.623178	344144.714743	40.295399
3344.662111	344674.017590	40.300416
3348.056249	345202.269356	40.305434
3351.617868	345722.492634	40.310452
3354.939491	346253.488222	40.315469
3358.033873	346787.840612	40.320487
3361.405579	347326.129945	40.325504
3364.966298	347870.274066	40.330522
3368.310599	348418.331326	40.335540
3371.508965	348969.021094	40.340557
3375.126432	349517.455888	40.345575
3378.576109	350070.862020	40.350592
3382.031411	350631.598139	40.355610
3385.646585	351185.220610	40.360628
3388.786510	351756.022191	40.365645
3392.686319	352299.637112	40.370663
3396.126727	352868.449971	40.375680
3399.641605	353421.963467	40.380698
3403.214736	353977.847994	40.385716
3406.807723	354542.760088	40.390733
3410.494788	355097.243819	40.395751
3414.074731	355665.267794	40.400768
3417.384015	356220.611296	40.405786
3421.215763	356773.784676	40.410804
3424.451036	357322.147435	40.415821
3427.815316	357880.052841	40.420839
3431.362812	358446.451300	40.425856
3435.038055	359009.878747	40.430874
3438.408142	359565.073611	40.435892
3441.141449	360141.809768	40.440909
3445.159452	360691.686100	40.445927
3449.064659	361253.629644	40.450944
3452.458515	361804.810057	40.455962
3457.002406	362337.249516	40.460980
3460.412840	362886.891819	40.465997
3464.158607	363417.034091	40.471015
3467.619880	363967.264659	40.476032
3471.119997	364494.616314	40.481050
3474.663668	365033.451403	40.486068
3478.137122	365559.373758	40.491085
3481.621570	366098.332428	40.496103
3485.030167	366641.077861	40.501120
3488.264433	367158.571188	40.506125
3491.391420	367639.209500	40.511130
3494.460037	368068.459892	40.516135
3497.150162	368456.042164	40.521140
3499.900239	368793.848693	40.526144
3502.388576	369068.753061	40.531149
3504.508240	369324.862326	40.536154
3506.048072	369525.270314	40.541159
3507.987972	369673.689856	40.546164
3509.343739	369781.089316	40.551168
3510.736141	369876.500245	40.556173
3512.085650	369927.854875	40.561178
3512.884952	369947.266904	40.566183
3513.698682	369944.823296	40.571188
3514.476231	369930.377510	40.576192
3515.134861	369879.239898	40.581197
3515.716571	369814.147536	40.586202
3515.773008	369742.345481	40.591207
3515.985099	369642.126959	40.596212
3516.242740	369537.830494	40.601216
3516.355233	369427.120211	40.606221
3516.525547	369303.196713	40.611226
3516.349833	369186.578223	40.616231
3516.648748	369046.224276	40.621236
3516.456669	368912.791144	40.626240
3516.149194	368771.997914	40.631245
3516.618665	368622.889328	40.636250
3515.748615	368481.471743	40.641255
3515.736892	368340.197864	40.646260
3515.496296	368192.014188	40.651264
3514.783606	368053.648764	40.656269
3514.850769	367909.486131	40.661274
3514.692930	367777.138116	40.666279
3514.521109	367630.671714	40.671284
3514.395283	367495.213893	40.676288
3513.731894	367364.750937	40.681293
3513.725807	367228.179364	40.686298
3513.411924	367109.719929	40.691303
3513.271911	366981.259358	40.696308
3512.888169	366845.713116	40.701312
3512.493761	366726.960084	40.706317
3512.482946	366610.792103	40.711322
3512.095896	366497.914490	40.716327
3511.899386	366379.409116	40.721332
3511.689507	366275.484142	40.726336
3511.304170	366171.993749	40.731341
3511.469256	366057.246754	40.736346
3511.090153	365958.181912	40.741351
3510.993210	365857.774661	40.746356
3510.946506	365745.553750	40.751360
3510.345297	365654.563302	40.756365
3510.062684	365570.697225	40.761370
3509.909279	365479.559303	40.766375
3510.038025	365390.870013	40.771380
3509.764531	365296.341333	40.776384
3509.451271	365224.870265	40.781389
3509.492604	365138.127981	40.786394
3509.225715	365061.331690	40.791399
3509.282321	364989.903552	40.796404
3509.290120	364913.623339	40.801408
3509.042478	364830.361004	40.806413
3509.153905	364749.000896	40.811418
3509.061915	364678.918821	40.816423
3508.607402	364603.347263	40.821428
3508.225619	364540.511305	40.826432
3508.171010	364476.834786	40.831437
3508.136746	364409.440192	40.836442
3507.650064	364350.462545	40.841447
3507.667907	364287.334069	40.846452
3507.884515	364236.361629	40.851456
3507.884417	364178.350027	40.856461
3507.513404	364113.069179	40.861466
3506.818722	364081.781465	40.866471
3507.157303	364016.210191	40.871476
3507.034426	363962.670401	40.876480
3507.034294	363924.886363	40.881485
3506.946897	363866.760951	40.886490
3506.464006	363834.828931	40.891495
3506.435873	363792.189417	40.896500
3506.576555	363737.106503	40.901504
3506.227183	363711.539734	40.906509
3506.363766	363674.013761	40.911514
3506.329749	363632.723563	40.916519
3506.240082	363595.691288	40.921524
3506.177480	363566.822260	40.926528
3505.942239	363544.214314	40.931533
3506.086255	363496.687486	40.936538
3505.879737	363472.166653	40.941543
3505.877763	363439.064232	40.946548
3505.968995	363403.428077	40.951552
3505.632422	363375.492789	40.956557
3505.795744	363342.211501	40.961562
3505.604214	363322.090069	40.966567
3505.870809	363298.130454	40.971572
3505.952495	363266.872113	40.976576
3505.298045	363245.246288	40.981581
3505.654853	363206.896348	40.986586
3505.614471	363197.946455	40.991591
3505.515949	363155.419258	40.996596
3505.939515	363145.785344	41.001600
3505.670367	363115.294807	41.006605
3505.678846	363076.440052	41.011610
3505.768647	363054.950921	41.016615
3505.746181	363019.485112	41.021620
3505.567866	362999.514118	41.026624
3505.284709	362973.860139	41.031629
3505.606948	362943.759439	41.036634
3505.530093	362918.836148	41.041639
3505.116840	362896.764918	41.046644
3505.274722	362868.573043	41.051648
3505.391075	362854.763854	41.056653
3505.382305	362828.175859	41.061658
3505.141763	362801.624491	41.066663
3505.112548	362778.907267	41.071668
3505.423885	362757.128530	41.076672
3505.063837	362736.397372	41.081677
3505.097064	362709.217446	41.086682
3505.146790	362692.339949	41.091687
3505.266811	362683.059263	41.096692
3505.392551	362660.699152	41.101696
3505.192835	362634.701016	41.106701
3505.156693	362612.391919	41.111706
3504.872899	362599.053029	41.116711
3505.027743	362572.311799	41.121716
3505.159415	362551.680934	41.126720
3504.983965	362539.978801	41.131725
3505.072844	362511.059724	41.136730
3505.289482	362490.924293	41.141735
3505.306324	362467.767077	41.146740
3505.098419	362452.914910	41.151744
3504.941376	362430.344948	41.156749
3505.018475	362403.514134	41.161754
3504.926707	362395.513666	41.166759
3505.042963	362358.524185	41.171764
3505.047321	362346.717242	41.176768
3504.630264	362332.305218	41.181773
3504.928022	362321.011669	41.186778
3504.986299	362299.374506	41.191783
3504.649329	362280.242519	41.196788
3504.792392	362266.937829	41.201792
3504.857455	362248.887287	41.206797
3504.834088	362222.352145	41.211802
3504.497623	362216.324138	41.216807
3504.651435	362206.274670	41.221812
3504.843933	362172.911601	41.226816
3504.642587	362172.078422	41.231821
3504.786028	362145.593201	41.236826
3504.905696	362131.172597	41.241831
3504.506590	362115.409090	41.246836
3504.619955	362111.167431	41.251840
3504.465110	362094.093056	41.256845
3504.600032	362075.471615	41.261850
3504.434711	362073.640388	41.266855
3504.578268	362052.651196	41.271860
3504.806222	362035.541726	41.276864
3504.686682	362017.927399	41.281869
3504.537689	362015.940918	41.286874
3504.747840	362000.589952	41.291879
3504.650519	361977.679546	41.296884
3504.514294	361961.390973	41.301888
3504.241282	361960.085666	41.306893
3504.692755	361930.854458	41.311898
3504.170726	361938.697823	41.316903
3504.098772	361912.653643	41.321908
3504.243920	361906.905686	41.326912
3504.312607	361903.536201	41.331917
3504.221191	361886.807953	41.336922
3504.323824	361879.285563	41.341927
3504.803646	361868.879144	41.346932
3504.262435	361852.832674	41.351936
3503.890993	361851.263029	41.356941
3504.799226	361825.292845	41.361946
3504.371250	361822.383549	41.366951
3504.445780	361813.313444	41.371956
3504.591681	361801.382207	41.376960
3504.313889	361797.863931	41.381965
3504.749736	361784.741823	41.386970
3504.476239	361767.151742	41.391975
3504.194537	361755.059089	41.396980
3504.798342	361741.503295	41.401984
3504.400328	361721.566488	41.406989
3504.617132	361706.850502	41.411994
3504.651986	361705.572851	41.416999
3504.640546	361688.704663	41.422004
3504.534102	361663.225590	41.427008
3504.229626	361660.423986	41.432013
3504.672779	361641.906315	41.437018
3504.422637	361623.600023	41.442023
3504.359867	361609.487999	41.447028
3504.480607	361596.593772	41.452032
3504.501124	361588.041066	41.457037
3504.543796	361562.309358	41.462042
3504.603751	361555.149896	41.467047
3504.525828	361533.737475	41.472052
3504.467811	361531.965597	41.477056
3504.056699	361514.855191	41.482061
3504.110204	361497.925778	41.487066
3504.296689	361493.214489	41.492071
3504.638537	361476.264929	41.497076
3504.589545	361470.903844	41.502080
3504.493382	361457.585856	41.507085
3504.504645	361443.512969	41.512090
3504.719699	361426.405319	41.517095
3504.341930	361405.421922	41.522100
3504.653445	361383.998755	41.527104
3504.222601	361368.418132	41.532109
3504.589639	361361.210094	41.537114
3504.288954	361358.967668	41.542119
3504.523147	361339.337876	41.547124
3504.471514	361324.740546	41.552128
3503.889436	361321.448456	41.557133
3504.427204	361306.452596	41.562138
3504.217507	361296.842083	41.567143
3504.326256	361290.769017	41.572148
3504.251693	361272.460277	41.577152
3504.032857	361260.306667	41.582157
3504.692997	361255.953045	41.587162
3504.365182	361242.493501	41.592167
3504.219329	361238.903434	41.597172
3504.184969	361227.763911	41.602176
3503.942211	361210.881233	41.607181
3504.361873	361201.476548	41.612186
3504.242774	361193.912768	41.617191
3504.082017	361183.276680	41.622196
3504.190355	361173.412300	41.627200
3503.838558	361157.208421	41.632205
3504.006008	361154.230396	41.637210
3504.142754	361150.493863	41.642215
3504.357197	361138.093606	41.647220
3504.348546	361130.868590	41.652224
3503.907752	361125.951089	41.657229
3503.953413	361107.038033	41.662234
3504.215139	361100.533631	41.667239
3504.079637	361094.499154	41.672244
3504.247039	361082.767901	41.677248
3504.013708	361084.382521	41.682253
3504.068556	361071.091442	41.687258
3503.777118	361059.254604	41.692263
3504.213418	361047.964295	41.697268
3504.343477	361043.643565	41.702272
3503.783018	361043.528721	41.707277
3504.020962	361022.625932	41.712282
3504.263019	361023.860053	41.717287
3503.854774	361011.863552	41.722292
3503.908837	360999.132377	41.727296
3503.811295	360991.056246	41.732301
3504.125723	360991.693680	41.737306
3503.744261	360981.983032	41.742311
3504.070457	360982.440487	41.747316
3504.195890	360972.522472	41.752320
3504.011219	360964.078429	41.757325
3504.184429	360944.178215	41.762330
3504.052689	360960.178939	41.767335
3504.219281	360942.111847	41.772340
3504.310524	360943.649714	41.777344
3504.249835	360929.537158	41.782349
3504.717834	360902.999931	41.787354
3504.270076	360904.852021	41.792359
3504.175829	360882.958422	41.797364
3504.450978	360875.026916	41.802368
3503.791187	360858.362715	41.807373
3504.142560	360845.889844	41.812378
3503.800411	360858.565051	41.817383
3504.099926	360839.560866	41.822388
3503.864721	360828.885577	41.827392
3503.918188	360823.991688	41.832397
3503.849748	360828.557381	41.837402
3504.007358	360817.794543	41.842407
3504.104198	360804.547642	41.847412
3504.188543	360790.692017	41.852416
3504.134555	360785.967786	41.857421
3504.053790	360780.840657	41.862426
3504.273367	360772.638018	41.867431
3504.318452	360766.574950	41.872436
3504.279310	360750.703187	41.877440
3503.943943	360753.733459	41.882445
3504.268914	360716.964155	41.887450
3503.802378	360719.531698	41.892455
3503.847972	360720.262529	41.897460
3504.363903	360696.745640	41.902464
3503.890710	360693.639857	41.907469
3504.107519	360689.000032	41.912474
3504.031910	360676.060261	41.917479
3504.192393	360669.139230	41.922484
3504.340020	360657.741792	41.927488
3503.943091	360640.577936	41.932493
3504.097775	360629.204822	41.937498
3504.031656	360635.296908	41.942503
3504.024827	360618.376721	41.947508
3504.132983	360605.636889	41.952512
3504.027987	360608.223618	41.957517
3504.084553	360586.026137	41.962522
3503.982203	360577.670794	41.967527
3503.858761	360572.906630	41.972532
3504.047350	360566.897186	41.977536
3503.647603	360559.046879	41.982541
3503.739465	360548.930518	41.987546
3503.739693	360559.770476	41.992551
3504.007453	360551.687410	41.997556
3503.883312	360532.851863	42.002560
3503.670817	360535.048460	42.007565
3504.237296	360530.760471	42.012570
3504.108326	360531.849696	42.017575
3504.103605	360518.669664	42.022580
3504.123634	360516.529169	42.027584
3503.620342	360503.555182	42.032589
3504.001510	360479.347011	42.037594
3503.762401	360481.522372	42.042599
3503.634433	360484.876112	42.047604
3504.210510	360484.327129	42.052608
3503.967698	360468.156677	42.057613
3504.063395	360454.121040	42.062618
3504.104252	360462.028333	42.067623
3504.129074	360434.975657	42.072628
3503.987487	360430.596034	42.077632
3503.593517	360431.014674	42.082637
3503.933748	360422.182201	42.087642
3504.058776	360404.681285	42.092647
3503.888345	360408.703335	42.097652
3504.281915	360395.333072	42.102656
3503.687502	360395.605281	42.107661
3503.914020	360378.775346	42.112666
3503.605658	360380.605419	42.117671
3503.999688	360379.143720	42.122676
3504.248316	360350.248961	42.127680
3503.634438	360349.124726	42.132685
3503.960138	360351.592487	42.137690
3503.874207	360339.163173	42.142695
3503.853490	360326.265520	42.147700
3503.980055	360327.238014	42.152704
3503.851815	360320.286240	42.157709
3504.090501	360308.976107	42.162714
3503.837601	360309.983146	42.167719
3504.173189	360295.578742	42.172724
3504.081180	360283.532062	42.177728
3503.783540	360279.202542	42.182733
3504.349288	360269.087541	42.187738
3503.795895	360259.531155	42.192743
3503.742355	360238.368756	42.197748
3503.753956	360234.499260	42.202752
3503.840685	360236.572227	42.207757
3503.908032	360240.276795	42.212762
3503.872644	360225.651114	42.217767
3503.765175	360216.227789	42.222772
3504.033977	360209.086000	42.227776
3503.323209	360220.496465	42.232781
3503.759381	360210.656396	42.237786
3503.610074	360200.323630	42.242791
3503.659673	360193.725411	42.247796
3503.769938	360195.438416	42.252800
3503.573295	360207.658211	42.257805
3503.970502	360192.556995	42.262810
3503.892711	360191.118990	42.267815
3503.926966	360173.097976	42.272820
3504.294745	360172.327461	42.277824
3503.605588	360165.489788	42.282829
3503.887875	360146.742512	42.287834
3503.793261	360141.795625	42.292839
3503.799339	360137.468968	42.297844
3503.804908	360140.216365	42.302848
3503.681026	360136.749970	42.307853
3504.009646	360118.402492	42.312858
3503.579217	360114.806437	42.317863
3503.775401	360110.526061	42.322868
3503.747475	360123.050002	42.327872
3503.562069	360112.570248	42.332877
3503.800148	360107.850667	42.337882
3503.998297	360106.267252	42.342887
3503.901608	360103.203691	42.347892
3503.932306	360089.941603	42.352896
3503.629386	360077.851878	42.357901
3503.887124	360067.302055	42.362906
3503.689770	360086.901328	42.367911
3503.782492	360074.850837	42.372916
3504.204256	360055.954245	42.377920
3503.735878	360046.816958	42.382925
3504.100298	360045.461714	42.387930
3503.770571	360038.058280	42.392935
3504.001809	360022.270761	42.397940
3503.927215	360031.748582	42.402944
3503.875084	360025.471776	42.407949
3503.847794	359987.230842	42.412954
3503.696013	359998.298527	42.417959
3503.741242	359987.604161	42.422964
3504.069763	359991.471027	42.427968
3503.582255	359983.583608	42.432973
3503.817151	359971.078031	42.437978
3503.880204	359957.963468	42.442983
3503.708232	359969.365150	42.447988
3503.820166	359964.767282	42.452992
3504.057866	359951.167077	42.457997
3503.912929	359925.387809	42.463002
3503.951005	359941.921840	42.468007
3503.878577	359934.248697	42.473012
3503.729098	359902.744772	42.478016
3503.608827	359907.674992	42.483021
3503.812136	359905.836294	42.488026
3503.939326	359905.231041	42.493031
3503.772872	359909.532411	42.498036
3503.668675	359890.108199	42.503040
3503.509576	359886.418339	42.508045
3503.918803	359884.623424	42.513050
3503.786769	359891.616638	42.518055
3503.585808	359868.772495	42.523060
3503.757778	359863.987004	42.528064
3503.497668	359860.160434	42.533069
3503.624468	359855.102176	42.538074
3503.659533	359862.959590	42.543079
3503.945786	359862.787220	42.548084
3504.146701	359835.579137	42.553088
3503.733783	359826.254918	42.558093
3503.872647	359824.350066	42.563098
3503.990328	359833.110485	42.568103
3503.840703	359811.912196	42.573108
3503.794768	359799.400080	42.578112
3503.707878	359805.444663	42.583117
3504.160897	359803.490145	42.588122
3503.852444	359787.177165	42.593127
3503.655321	359779.320142	42.598132
3504.092534	359767.902158	42.603136
3503.733197	359766.279636	42.608141
3503.749875	359748.413919	42.613146
3503.767439	359743.703718	42.618151
3503.751590	359746.123723	42.623156
3503.914113	359743.044606	42.628160
3503.817219	359727.054405	42.633165
3503.912915	359726.886713	42.638170
3503.829207	359718.655504	42.643175
3503.894247	359718.289090	42.648180
3503.884442	359700.834681	42.653184
3503.815665	359697.715789	42.658189
3504.137410	359687.893704	42.663194
3504.119367	359675.987855	42.668199
3503.386733	359675.772995	42.673204
3503.849555	359659.592499	42.678208
3503.657515	359673.033119	42.683213
3503.631572	359657.337032	42.688218
3503.755912	359671.134774	42.693223
3503.675886	359656.694101	42.698228
3504.060140	359636.632750	42.703232
3503.634903	359647.234822	42.708237
3503.486083	359641.838422	42.713242
3503.747103	359638.921850	42.718247
3503.718640	359627.043083	42.723252
3503.929218	359614.821167	42.728256
3503.628184	359610.593908	42.733261
3503.599952	359612.863200	42.738266
3503.782647	359612.630862	42.743271
3503.659313	359598.247911	42.748276
3503.776823	359577.007286	42.753280
3503.417777	359590.703348	42.758285
3503.707203	359585.721136	42.763290
3503.726657	359590.756531	42.768295
3503.577152	359585.767373	42.773300
3503.640017	359567.894287	42.778304
3503.605250	359569.350334	42.783309
3503.768281	359559.197067	42.788314
3503.854214	359566.257654	42.793319
3503.754810	359563.525289	42.798324
3503.924300	359550.521019	42.803329
3503.875962	359547.322548	42.808333
3503.641127	359539.242432	42.813338
3503.942704	359534.131062	42.818343
3503.941038	359533.342606	42.823348
3503.799107	359514.356795	42.828353
3503.549771	359512.487858	42.833357
3503.942918	359499.753571	42.838362
3503.998990	359501.627846	42.843367
3503.856409	359491.192079	42.848372
3504.169665	359475.951234	42.853377
3503.856210	359472.260299	42.858381
3503.920196	359453.318248	42.863386
3504.011696	359448.163743	42.868391
3503.469131	359448.682222	42.873396
3503.882786	359446.479450	42.878401
3504.058951	359441.642361	42.883405
3504.014202	359417.246529	42.888410
3503.678375	359419.717138	42.893415
3503.750203	359419.782236	42.898420
3503.404632	359384.695596	42.903425
3503.523025	359391.114918	42.908429
3503.409528	359379.478551	42.913434
3503.653524	359381.552138	42.918439
3503.701634	359387.295520	42.923444
3503.631896	359386.263360	42.928449
3503.762364	359393.927643	42.933453
3503.724449	359381.872186	42.938458
3503.741646	359366.372756	42.943463
3503.427518	359366.855121	42.948468
3503.616702	359353.007955	42.953473
3503.902733	359370.190032	42.958477
3503.842947	359361.013465	42.963482
3503.730625	359347.595660	42.968487
3503.593831	359335.326806	42.973492
3503.591993	359335.428997	42.978497
3503.704365	359338.363125	42.983501
3503.690352	359339.892237	42.988506
3503.765600	359324.688972	42.993511
3503.414987	359311.741418	42.998516
3503.805519	359313.053896	43.003521
3503.513852	359320.479572	43.008525
3503.701013	359310.958598	43.013530
3503.532814	359320.425911	43.018535
3503.643005	359317.838521	43.023540
3503.783542	359295.118243	43.028545
3503.747746	359290.569113	43.033549
3503.813500	359296.055253	43.038554
3503.596636	359294.155727	43.043559
3503.393639	359300.244175	43.048564
3503.858665	359293.961853	43.053569
3503.466342	359269.824467	43.058573
3503.675845	359259.231202	43.063578
3503.653363	359260.354513	43.068583
3503.994484	359272.235063	43.073588
3503.893452	359260.622143	43.078593
3503.726859	359263.244129	43.083597
3504.026257	359241.262103	43.088602
3503.931145	359252.829927	43.093607
3503.608100	359241.608351	43.098612
3504.037726	359224.033405	43.103617
3503.919422	359222.830795	43.108621
3503.920815	359233.798099	43.113626
3503.892757	359209.959346	43.118631
3503.789204	359191.450823	43.123636
3504.106724	359186.769487	43.128641
3503.846186	359190.525972	43.133645
3504.172422	359164.442791	43.138650
3503.896773	359159.575317	43.143655
3503.695885	359152.380396	43.148660
3503.805090	359150.658333	43.153665
3503.515700	359122.484059	43.158669
3503.574270	359113.008823	43.163674
3503.617388	359113.078460	43.168679
3503.610783	359119.772045	43.173684
3503.545283	359125.558866	43.178689
3503.356650	359123.120494	43.183693
3503.580143	359116.545530	43.188698
3503.581521	359110.514610	43.193703
3503.451391	359102.646886	43.198708
3503.577177	359089.038686	43.203713
3503.694976	359094.465728	43.208717
3503.629895	359080.073413	43.213722
3503.657088	359101.749644	43.218727
3503.491423	359102.335773	43.223732
3503.641434	359101.192526	43.228737
3503.584434	359077.078372	43.233741
3503.551095	359062.502908	43.238746
3503.534016	359075.610675	43.243751
3503.266513	359061.555715	43.248756
3503.620338	359066.792766	43.253761
3503.381264	359074.591862	43.258765
3503.569470	359071.050604	43.263770
3503.469601	359076.588400	43.268775
3503.560619	359082.248695	43.273780
3504.069223	359050.283925	43.278785
3503.608235	359052.647106	43.283789
3503.778769	359051.297042	43.288794
3504.024536	359041.232373	43.293799
3503.628514	359042.872781	43.298804
3503.707657	359024.920582	43.303809
3503.949264	359031.244133	43.308813
3503.759520	359019.772413	43.313818
3503.395754	359029.906864	43.318823
3503.271606	359023.692206	43.323828
3503.745093	359013.413404	43.328833
3503.431826	358998.093333	43.333837
3503.483958	358996.482074	43.338842
3503.694510	359005.100727	43.343847
3503.894134	358990.564751	43.348852
3503.619176	358995.366840	43.353857
3503.488558	358980.043334	43.358861
3503.477688	358965.464289	43.363866
3503.362348	358964.184864	43.368871
3503.282225	358968.803473	43.373876
3503.667066	358964.238705	43.378881
3503.372011	358976.169010	43.383885
3503.616341	358969.539839	43.388890
3503.684482	358973.931436	43.393895
3503.898397	358976.824086	43.398900
3503.562904	358959.878938	43.403905
3503.325984	358949.916007	43.408909
3503.445347	358935.952528	43.413914
3503.547961	358942.323511	43.418919
3503.447876	358945.036785	43.423924
3503.725772	358944.916627	43.428929
3503.703792	358942.757258	43.433933
3503.375104	358940.086552	43.438938
3503.562882	358916.391659	43.443943
3503.523599	358921.538195	43.448948
3503.648852	358910.627368	43.453953
3503.460865	358925.492563	43.458957
3503.700262	358911.840906	43.463962
3503.968213	358924.267488	43.468967
3503.424028	358912.113826	43.473972
3503.806755	358899.406477	43.478977
3503.661193	358894.747430	43.483981
3503.420610	358896.007017	43.488986
3503.851710	358890.696977	43.493991
3503.698890	358894.512795	43.498996
3503.765323	358875.646473	43.504001
3503.579258	358872.469731	43.509005
3503.900600	358857.583667	43.514010
3503.803514	358865.207669	43.519015
3503.565794	358866.543143	43.524020
3503.879046	358862.651296	43.529025
3503.796031	358838.871943	43.534029
3503.602495	358832.515550	43.539034
3503.750708	358839.769970	43.544039
3503.520977	358832.783134	43.549044
3503.610588	358834.270433	43.554049
3503.459304	358831.978821	43.559053
3503.624356	358814.979935	43.564058
3503.645477	358811.185161	43.569063
3503.463079	358823.886539	43.574068
3503.701349	358811.939957	43.579073
3503.498689	358817.519479	43.584077
3503.385479	358821.837974	43.589082
3503.421939	358816.234064	43.594087
3503.509819	358790.086578	43.599092
3503.571277	358787.583205	43.604097
3503.818521	358789.147371	43.609101
3504.012385	358785.859665	43.614106
3503.811743	358787.749106	43.619111
3503.532051	358774.510283	43.624116
3503.772996	358749.687250	43.629121
3503.876955	358756.541531	43.634125
3503.639001	358746.884083	43.639130
3503.660700	358768.688564	43.644135
3503.280563	358736.177034	43.649140
3503.743650	358722.744427	43.654145
3503.463466	358730.422844	43.659149
3503.757495	358726.661258	43.664154
3503.574965	358730.736253	43.669159
3503.483777	358731.946778	43.674164
3503.488132	358720.775109	43.679169
3503.844100	358732.220849	43.684173
3503.762340	358712.843513	43.689178
3503.334685	358710.722822	43.694183
3503.168808	358699.654400	43.699188
3503.640413	358700.419698	43.704193
3503.311437	358707.011624	43.709197
3503.718120	358707.176464	43.714202
3503.468013	358700.803552	43.719207
3503.356374	358709.676767	43.724212
3503.817790	358700.035976	43.729217
3503.416489	358685.722146	43.734221
3503.332740	358678.813996	43.739226
3503.720710	358671.398674	43.744231
3503.550746	358672.825229	43.749236
3503.563139	358664.604095	43.754241
3503.488263	358679.553269	43.759245
3503.392114	358678.194462	43.764250
3503.624222	358686.300829	43.769255
3503.400287	358673.053163	43.774260
3503.425337	358660.783999	43.779265
3503.490277	358649.221035	43.784269
3503.616947	358651.923923	43.789274
3503.580616	358645.033719	43.794279
3503.438651	358651.316172	43.799284
3503.623364	358655.587582	43.804289
3503.778389	358661.975762	43.809293
3503.620760	358640.930908	43.814298
3503.903885	358615.235949	43.819303
3503.423074	358631.877906	43.824308
3503.442280	358630.984349	43.829313
3503.432709	358638.390977	43.834317
3503.578594	358625.848233	43.839322
3503.234091	358629.490802	43.844327
3503.555235	358630.661590	43.849332
3503.712331	358608.065607	43.854337
3503.506400	358598.428513	43.859341
3503.499764	358602.017669	43.864346
3503.821414	358591.075722	43.869351
3503.629373	358615.865886	43.874356
3503.756144	358604.547603	43.879361
3503.638136	358590.290745	43.884365
3503.398392	358573.890154	43.889370
3503.337959	358570.108254	43.894375
3503.405272	358576.383079	43.899380
3503.499750	358571.126223	43.904385
3503.397596	358577.605966	43.909389
3503.322025	358577.847049	43.914394
3503.751107	358573.071677	43.919399
3503.477871	358587.874112	43.924404
3503.989133	358575.833420	43.929409
3503.627367	358557.721734	43.934413
3503.359697	358538.246486	43.939418
3503.451056	358553.474779	43.944423
3503.469341	358550.825538	43.949428
3503.819419	358539.675511	43.954433
3503.708356	358555.241167	43.959437
3503.214735	358543.384781	43.964442
3503.318363	358524.894145	43.969447
3503.292853	358523.040677	43.974452
3503.444516	358515.611798	43.979457
3503.268999	358521.670551	43.984461
3503.278728	358516.223514	43.989466
3503.343780	358522.142447	43.994471
3503.267034	358524.164992	43.999476
3503.370164	358522.189399	44.004481
3503.547883	358532.645496	44.009485
3503.394946	358542.314121	44.014490
3503.607430	358528.463038	44.019495
3503.163696	358540.620528	44.024500
3503.249322	358532.387794	44.029505
3503.554730	358534.706177	44.034509
3503.720991	358543.611828	44.039514
3503.937086	358516.095247	44.044519
3503.653518	358521.967508	44.049524
3503.716622	358503.101569	44.054529
3503.629467	358508.917333	44.059533
3503.455213	358518.105844	44.064538
3503.557843	358516.257564	44.069543
3503.424265	358497.855313	44.074548
3503.747078	358478.846518	44.079553
3503.285319	358479.861167	44.084557
3503.263724	358474.597205	44.089562
3503.526387	358474.861156	44.094567
3503.612986	358479.020858	44.099572
3503.834496	358475.448845	44.104577
3503.776175	358474.771116	44.109581
3503.895297	358459.280731	44.114586
3503.879981	358453.328709	44.119591
3503.614519	358443.115719	44.124596
3504.010981	358437.963788	44.129601
3503.704360	358430.225645	44.134605
3503.709159	358417.119876	44.139610
3504.099184	358400.288855	44.144615
3503.398080	358419.128693	44.149620
3503.770584	358412.453736	44.154625
3503.308232	358398.607517	44.159629
3503.302216	358390.541929	44.164634
3503.384968	358392.335688	44.169639
3503.504844	358392.724001	44.174644
3503.841738	358390.202509	44.179649
3503.815603	358403.795378	44.184653
3503.541543	358395.263229	44.189658
3503.778070	358399.195660	44.194663
3503.587061	358385.230199	44.199668
3503.624694	358358.937746	44.204673
3503.479907	358375.170410	44.209677
3503.382385	358369.587631	44.214682
3503.387522	358358.492096	44.219687
3503.497716	358360.943137	44.224692
3503.463071	358369.778794	44.229697
3503.594310	358381.947211	44.234701
3503.547420	358359.536045	44.239706
3503.564612	358336.478565	44.244711
3503.461053	358341.304514	44.249716
3503.821040	358334.682419	44.254721
3503.869355	358339.484358	44.259725
3503.552279	358340.654264	44.264730
3503.614541	358348.278601	44.269735
3503.602267	358326.370884	44.274740
3503.407496	358312.431444	44.279745
3503.649630	358308.499903	44.284749
3503.743739	358311.996812	44.289754
3503.710715	358311.442316	44.294759
3503.407522	358312.381005	44.299764
3503.734815	358301.081845	44.304769
3503.422939	358289.960072	44.309773
3503.514976	358278.316395	44.314778
3503.704715	358288.210811	44.319783
3503.640853	358278.907450	44.324788
3503.615112	358276.774093	44.329793
3503.564448	358297.903157	44.334797
3503.484550	358278.856164	44.339802
3503.711319	358255.969089	44.344807
3503.392405	358255.510684	44.349812
3503.592804	358253.036211	44.354817
3503.554284	358255.765237	44.359821
3503.692224	358247.066140	44.364826
3503.766191	358248.301461	44.369831
3503.454773	358244.050277	44.374836
3503.514635	358230.096004	44.379841
3503.404872	358220.367291	44.384845
3503.295187	358219.977595	44.389850
3503.404910	358223.141232	44.394855
3502.982585	358217.991490	44.399860
3503.672880	358222.768287	44.404865
3503.692896	358214.342296	44.409869
3503.479126	358224.147836	44.414874
3503.470787	358217.711191	44.419879
3503.593610	358220.567394	44.424884
3503.739741	358211.434397	44.429889
3503.324383	358212.747078	44.434893
3503.222998	358204.823771	44.439898
3503.803345	358195.902041	44.444903
3503.378366	358211.161177	44.449908
3503.682006	358200.400119	44.454913
3503.420230	358205.403776	44.459917
3503.424565	358203.087532	44.464922
3503.711576	358181.590482	44.469927
3503.472203	358181.017713	44.474932
3503.995879	358174.751423	44.479937
3503.726781	358171.307845	44.484941
3503.325629	358171.269592	44.489946
3503.607668	358165.499548	44.494951
3503.439700	358172.727712	44.499956
3503.811498	358167.121607	44.504961
3503.814226	358155.262998	44.509965
3503.490620	358137.959427	44.514970
3503.467505	358147.607605	44.519975
3503.348893	358134.266802	44.524980
3503.787080	358142.798725	44.529985
3503.382022	358141.743210	44.534989
3503.424446	358140.973208	44.539994
3503.425025	358112.828851	44.544999
3503.420700	358114.178341	44.550004
3503.490745	358114.421852	44.555009
3503.696335	358106.602680	44.560013
3503.498864	358115.667701	44.565018
3503.934109	358115.420877	44.570023
3503.600964	358101.223336	44.575028
3503.908627	358085.626684	44.580033
3503.647568	358079.458998	44.585037
3503.274969	358075.242919	44.590042
3503.896188	358072.472885	44.595047
3503.588564	358079.494118	44.600052
3503.662415	358075.232904	44.605057
3503.638639	358056.253294	44.610061
3503.584955	358037.202063	44.615066
3503.485199	358048.872694	44.620071
3503.742012	358056.110060	44.625076
3503.655194	358033.679611	44.630081
3503.547778	358048.761357	44.635085
3503.404055	358045.730548	44.640090
3503.473834	358021.163232	44.645095
3503.597719	358021.779937	44.650100
3503.701696	358009.065533	44.655105
3503.403680	358015.398186	44.660109
3503.200468	358024.336896	44.665114
3503.372190	358016.141359	44.670119
3503.426961	358029.441622	44.675124
3503.737460	358026.568026	44.680129
3503.591808	358023.308499	44.685133
3503.450545	358015.289677	44.690138
3503.866881	357987.588461	44.695143
3503.547285	357998.250530	44.700148
3503.475040	357985.258614	44.705153
3503.587551	357998.066264	44.710157
3503.444082	357997.172966	44.715162
3503.910641	357995.496155	44.720167
3503.170226	357978.716471	44.725172
3503.425461	357971.322029	44.730177
3503.679409	357962.095600	44.735181
3503.360983	357974.767808	44.740186
3503.350400	357962.275080	44.745191
3503.568235	357963.640346	44.750196
3503.522237	357964.462039	44.755201
3503.442927	357972.261499	44.760205
3503.730432	357956.947911	44.765210
3503.548511	357956.951340	44.770215
3503.206848	357950.618251	44.775220
3503.318569	357942.559422	44.780225
3503.633933	357949.965678	44.785229
3503.152398	357946.275751	44.790234
3503.380007	357946.697930	44.795239
3503.431225	357955.927240	44.800244
3503.363259	357950.950471	44.805249
3503.399846	357946.415220	44.810253
3503.727808	357942.928128	44.815258
3503.689064	357949.779635	44.820263
3503.373372	357953.265016	44.825268
3503.708635	357936.824201	44.830273
3503.714487	357925.906585	44.835277
3503.067718	357916.008238	44.840282
3503.565924	357921.222587	44.845287
3503.339174	357914.133360	44.850292
3503.573635	357915.521446	44.855297
3503.464380	357910.067705	44.860301
3503.412353	357928.219831	44.865306
3503.592647	357917.121953	44.870311
3503.061323	357939.701304	44.875316
3503.404761	357925.371301	44.880321
3503.536310	357927.615410	44.885325
3503.611712	357903.352511	44.890330
3503.590735	357897.783024	44.895335
3503.404584	357895.369645	44.900340
3503.556762	357885.268642	44.905345
3503.824110	357892.300790	44.910349
3503.376942	357894.534605	44.915354
3503.542326	357899.725232	44.920359
3503.328796	357888.994974	44.925364
3503.269669	357861.801457	44.930369
3503.641391	357865.763451	44.935373
3503.005584	357870.775380	44.940378
3503.325653	357862.225552	44.945383
3503.719126	357866.642156	44.950388
3503.470771	357862.660887	44.955393
3503.195953	357872.298018	44.960397
3503.454404	357872.638980	44.965402
3503.576213	357858.751150	44.970407
3503.210389	357882.093224	44.975412
3503.255569	357873.994010	44.980417
3503.560548	357883.895735	44.985421
3503.501476	357880.571616	44.990426
3503.490582	357875.484028	44.995431
3503.296107	357868.033432	45.000436
3503.596889	357853.404786	45.005441
3503.316125	357849.988477	45.010445
3503.452261	357855.998041	45.015450
3503.473460	357841.998877	45.020455
3503.489496	357853.473118	45.025460
3503.345719	357851.154826	45.030465
3503.484513	357860.701122	45.035469
3503.276281	357860.225214	45.040474
3503.366970	357865.122289	45.045479
3503.218640	357861.506913	45.050484
3503.676612	357859.602432	45.055489
3503.487933	357845.890920	45.060493
3503.361819	357840.134471	45.065498
3503.348287	357822.654533	45.070503
3503.251779	357831.296490	45.075508
3503.356070	357832.603369	45.080513
3503.778762	357829.941049	45.085517
3503.608111	357826.736354	45.090522
3504.077802	357824.728230	45.095527
3503.674628	357817.666881	45.100532
3503.704469	357805.702112	45.105537
3503.891664	357798.649215	45.110541
3503.282868	357809.382492	45.115546
3503.881379	357788.065048	45.120551
3503.500874	357797.718901	45.125556
3503.435428	357783.249922	45.130561
3503.399120	357764.348522	45.135565
3503.342318	357760.107937	45.140570
3503.196432	357759.723961	45.145575
3503.219655	357763.461141	45.150580
3503.352460	357758.757977	45.155585
3503.242915	357762.567041	45.160589
3503.334749	357762.578085	45.165594
3503.600915	357761.314655	45.170599
3503.445894	357763.425947	45.175604
3503.649780	357767.643509	45.180609
3503.735727	357777.834355	45.185613
3503.710041	357769.313725	45.190618
3503.762880	357749.609363	45.195623
3503.623218	357746.730578	45.200628
3503.567183	357739.436206	45.205633
3503.721773	357751.524746	45.210637
3503.212804	357743.385883	45.215642
3503.652700	357744.283446	45.220647
3503.504129	357736.621995	45.225652
3503.687750	357714.810273	45.230657
3503.372327	357715.369199	45.235661
3503.384834	357701.931207	45.240666
3503.720711	357707.883765	45.245671
3503.654574	357711.482392	45.250676
3503.860659	357701.652749	45.255681
3503.924651	357692.787114	45.260685
3503.382237	357682.999459	45.265690
3503.652801	357675.704339	45.270695
3503.767257	357666.652591	45.275700
3503.702218	357670.480073	45.280705
3503.665076	357671.122241	45.285709
3503.411919	357657.395424	45.290714
3503.452497	357634.206682	45.295719
3503.476779	357647.053819	45.300724
3503.447777	357639.144425	45.305729
3503.384008	357644.829357	45.310733
3503.153660	357635.628538	45.315738
3503.511090	357644.224209	45.320743
3503.461111	357642.883521	45.325748
3503.615569	357643.826212	45.330753
3503.401450	357645.336119	45.335757
3503.763624	357637.288540	45.340762
3503.469900	357621.990396	45.345767
3503.152664	357619.623175	45.350772
3503.739281	357613.804915	45.355777
3503.665542	357611.271961	45.360781
3503.525404	357615.416688	45.365786
3503.591788	357621.208283	45.370791
3503.582228	357618.512499	45.375796
3503.626422	357605.603865	45.380801
3503.657752	357595.165646	45.385805
3503.586729	357580.951962	45.390810
3503.641782	357580.587112	45.395815
3503.350101	357593.713240	45.400820
3503.338457	357585.979224	45.405825
3503.489524	357588.907340	45.410829
3503.572972	357588.385316	45.415834
3503.250013	357574.516828	45.420839
3503.284304	357553.288483	45.425844
3503.056783	357555.563930	45.430849
3503.226316	357562.662483	45.435853
3503.442783	357569.880853	45.440858
3503.378153	357555.437125	45.445863
3503.299175	357563.363833	45.450868
3503.546463	357557.293845	45.455873
3503.680053	357552.030698	45.460877
3503.225056	357561.085639	45.465882
3503.568214	357549.071275	45.470887
3503.413765	357566.705333	45.475892
3503.345660	357568.243052	45.480897
3503.654277	357576.413848	45.485901
3503.402942	357564.340791	45.490906
3503.658876	357559.669037	45.495911
3503.501956	357534.399347	45.500916
3503.852244	357532.384641	45.505921
3503.605151	357531.533164	45.510925
3503.220726	357534.520495	45.515930
3503.394517	357528.233097	45.520935
3503.564398	357541.108137	45.525940
3503.672922	357527.807603	45.530945
3503.513418	357519.689795	45.535949
3503.569567	357517.034513	45.540954
3503.974357	357504.934052	45.545959
3503.606684	357514.687722	45.550964
3503.552200	357515.129054	45.555969
3503.729353	357514.464979	45.560973
3503.405125	357501.258301	45.565978
3503.712651	357483.345776	45.570983
3503.347781	357492.004771	45.575988
3503.575983	357477.031227	45.580993
3503.480876	357474.094487	45.585997
3503.582755	357475.274519	45.591002
3503.647864	357465.976063	45.596007
3503.375619	357474.238708	45.601012
3503.419694	357475.376985	45.606017
3503.249221	357459.295886	45.611021
3503.154764	357445.289447	45.616026
3503.409263	357438.378542	45.621031
3503.024398	357442.663762	45.626036
3503.248413	357442.857488	45.631041
3503.261225	357439.674658	45.636045
3503.000839	357452.032455	45.641050
3503.593045	357446.569555	45.646055
3503.220358	357448.791614	45.651060
3503.180641	357451.444532	45.656065
3503.394827	357447.619131	45.661069
3503.578289	357455.046313	45.666074
3503.385508	357456.374720	45.671079
3502.999441	357453.025926	45.676084
3503.159726	357459.006274	45.681089
3503.376247	357451.643323	45.686093
3503.238963	357468.485834	45.691098
3503.719885	357458.281876	45.696103
3503.122685	357472.881388	45.701108
3503.464958	357458.424198	45.706113
3503.419103	357465.963975	45.711117
3503.114928	357467.131861	45.716122
3503.218752	357465.995879	45.721127
3503.246978	357473.498495	45.726132
3503.469597	357465.091241	45.731137
3503.291488	357487.055115	45.736141
3503.381977	357480.908118	45.741146
3503.691933	357471.291033	45.746151
3503.408068	357454.922491	45.751156
3503.365661	357442.740031	45.756161
3503.786015	357438.576667	45.761165
3503.232722	357438.969623	45.766170
3503.632767	357449.187222	45.771175
3503.437771	357450.719558	45.776180
3503.790423	357437.558535	45.781185
3503.715754	357448.411026	45.786189
3503.244916	357434.820350	45.791194
3503.400045	357420.876235	45.796199
3503.326587	357416.027517	45.801204
3503.508840	357413.937582	45.806209
3503.547270	357418.588489	45.811213
3503.761504	357409.648157	45.816218
3503.647668	357413.025321	45.821223
3503.464985	357417.965658	45.826228
3503.683537	357410.678722	45.831233
3503.894358	357385.478056	45.836237
3503.513345	357388.337618	45.841242
3503.504784	357377.193134	45.846247
3503.232965	357372.833824	45.851252
3503.341745	357383.097484	45.856257
3503.596629	357378.756695	45.861261
3503.509351	357388.542402	45.866266
3503.460485	357384.885820	45.871271
3503.156478	357385.799208	45.876276
3503.483514	357383.711830	45.881281
3503.543204	357370.648000	45.886285
3503.188442	357356.428215	45.891290
3503.551393	357349.092993	45.896295
3503.451812	357348.523561	45.901300
3503.266765	357350.741407	45.906305
3503.485526	357355.745522	45.911309
3503.318483	357355.899282	45.916314
3503.600186	357353.157437	45.921319
3503.247999	357364.664558	45.926324
3503.834014	357350.932223	45.931329
3503.613707	357357.405359	45.936333
3503.394145	357336.904134	45.941338
3503.514420	357323.449003	45.946343
3503.458747	357330.735878	45.951348
3503.583915	357325.626723	45.956353
3503.453955	357325.698279	45.961357
3503.787149	357323.737161	45.966362
3503.624874	357319.818582	45.971367
3503.427607	357325.422867	45.976372
3503.535956	357299.780304	45.981377
3503.644222	357298.847195	45.986381
3503.242847	357294.737388	45.991386
3503.513523	357296.094318	45.996391
3503.694017	357287.846379	46.001396
3503.772445	357291.778446	46.006401
3503.527806	357303.599394	46.011405
3503.318677	357291.875861	46.016410
3503.564999	357294.203645	46.021415
3503.463395	357270.222894	46.026420
3503.312694	357270.832125	46.031425
3503.815505	357268.437031	46.036429
3503.579849	357267.278372	46.041434
3503.636599	357264.343059	46.046439
3503.296956	357259.994462	46.051444
3503.308077	357269.459267	46.056449
3503.639437	357265.233615	46.061453
3503.448092	357249.257538	46.066458
3503.468491	357232.688136	46.071463
3503.253608	357234.096385	46.076468
3503.440410	357233.939730	46.081473
3503.754436	357228.240863	46.086477
3503.430240	357232.007561	46.091482
3503.503225	357235.991388	46.096487
3503.309972	357232.993808	46.101492
3503.475433	357236.174143	46.106497
3503.390679	357241.506175	46.111501
3503.333104	357238.436250	46.116506
3503.575783	357221.068279	46.121511
3503.282238	357223.150599	46.126516
3503.137452	357211.645902	46.131521
3503.540591	357210.869753	46.136525
3503.670822	357210.696595	46.141530
3503.495865	357187.541720	46.146535
3503.409116	357203.460222	46.151540
3503.770077	357197.881169	46.156545
3503.606113	357209.129541	46.161549
3503.334051	357200.724107	46.166554
3503.431259	357198.265896	46.171559
3503.126614	357186.277516	46.176564
3503.348300	357178.023047	46.181569
3503.366322	357171.989258	46.186573
3503.341973	357179.093071	46.191578
3503.531722	357165.016174	46.196583
3503.481319	357164.947914	46.201588
3503.441197	357171.367140	46.206593
3503.418003	357169.156990	46.211597
3503.343666	357180.136724	46.216602
3503.662626	357173.266486	46.221607
3503.801556	357185.128613	46.226612
3503.605323	357176.558501	46.231617
3503.729115	357153.992567	46.236621
3503.365107	357155.042682	46.241626
3503.598918	357131.568682	46.246631
3503.590580	357141.520090	46.251636
3503.569287	357141.472677	46.256641
3503.434276	357142.893749	46.261645
3503.236817	357150.050381	46.266650
3503.700148	357136.871782	46.271655
3503.491025	357121.356529	46.276660
3503.166658	357112.145028	46.281665
3503.400192	357118.088389	46.286669
3503.529273	357115.243422	46.291674
3503.515933	357115.754597	46.296679
3503.487120	357115.123079	46.301684
3503.448611	357113.424298	46.306689
3503.598572	357101.007762	46.311693
3503.547750	357117.963960	46.316698
3503.576721	357098.492141	46.321703
3503.310218	357093.012275	46.326708
3503.604850	357085.178865	46.331713
3503.377600	357075.697529	46.336717
3503.429280	357079.811974	46.341722
3503.412369	357084.471662	46.346727
3503.132361	357077.390735	46.351732
3503.234843	357083.329371	46.356737
3503.543933	357081.957348	46.361741
3503.288470	357097.571739	46.366746
3503.360665	357086.363527	46.371751
3503.368448	357094.581964	46.376756
3503.223544	357088.930188	46.381761
3503.077737	357092.210638	46.386765
3503.316713	357098.102246	46.391770
3503.612220	357083.270628	46.396775
3503.272595	357109.153675	46.401780
3503.329326	357095.530396	46.406785
3503.772579	357083.143830	46.411789
3503.448507	357069.071795	46.416794
3503.612700	357072.913978	46.421799
3503.719641	357076.510737	46.426804
3503.663366	357075.883560	46.431809
3503.650974	357073.697145	46.436813
3503.374105	357067.531832	46.441818
3503.455175	357030.900104	46.446823
3503.252894	357042.841655	46.451828
3503.320873	357032.346629	46.456833
3503.603452	357033.319972	46.461837
3503.433861	357044.900089	46.466842
3503.486167	357033.567772	46.471847
3503.618931	357030.187820	46.476852
3503.716341	357038.137620	46.481857
3503.742586	357034.774508	46.486861
3503.419587	357016.554337	46.491866
3503.609416	357002.986333	46.496871
3503.505189	357005.674921	46.501876
3503.324395	356992.623564	46.506881
3503.713145	357001.672452	46.511885
3503.411603	357005.155662	46.516890
3503.562568	357000.042395	46.521895
3503.428856	357009.581041	46.526900
3502.926449	357006.632323	46.531905
3503.369352	357008.012929	46.536909
3503.265005	357014.035167	46.541914
3503.525198	357006.690694	46.546919
3503.306085	356989.293859	46.551924
3503.465746	356977.308367	46.556929
3503.345843	356968.446229	46.561933
3503.209102	356964.294557	46.566938
3503.542694	356970.552935	46.571943
3503.548677	356976.455945	46.576948
3503.752300	356977.289086	46.581953
3503.528481	356978.367936	46.586957
3503.543343	356980.274271	46.591962
3503.624775	356968.937334	46.596967
3503.495744	356961.298122	46.601972
3503.115115	356956.014417	46.606977
3503.839119	356934.295055	46.611981
3503.171731	356949.338425	46.616986
3503.354458	356937.705544	46.621991
3502.987057	356949.571431	46.626996
3503.498607	356944.019438	46.632001
3503.292560	356948.429116	46.637005
3503.084636	356955.053031	46.642010
3503.525633	356944.193643	46.647015
3503.602496	356953.648114	46.652020
3503.344881	356945.418486	46.657025
3503.606065	356950.441382	46.662029
3503.236614	356957.218071	46.667034
3503.445172	356953.724340	46.672039
3503.153565	356932.699940	46.677044
3503.276259	356923.773993	46.682049
3503.725684	356914.643704	46.687053
3503.446197	356923.162061	46.692058
3503.623732	356908.679861	46.697063
3503.633018	356921.555003	46.702068
3503.248431	356918.485862	46.707073
3503.714267	356920.422692	46.712077
3503.603395	356918.048259	46.717082
3503.705879	356912.637277	46.722087
3503.094096	356889.449533	46.727092
3503.238570	356881.563488	46.732097
3503.666741	356894.550547	46.737101
3503.269239	356885.834072	46.742106
3503.484702	356888.268543	46.747111
3503.734178	356886.447883	46.752116
3503.594969	356882.881889	46.757121
3503.814733	356886.995225	46.762125
3503.323180	356889.032520	46.767130
3503.427091	356856.875836	46.772135
3503.423758	356859.243109	46.777140
3503.444513	356847.177757	46.782145
3503.204103	356858.896351	46.787149
3503.168832	356861.115987	46.792154
3503.536851	356852.405719	46.797159
3503.419547	356854.103924	46.802164
3503.220124	356858.563458	46.807169
3503.512624	356848.287374	46.812173
3503.344467	356853.912557	46.817178
3503.553543	356858.460195	46.822183
3503.482931	356856.232080	46.827188
3503.579294	356861.357385	46.832193
3503.566294	356841.179567	46.837197
3503.569423	356831.865344	46.842202
3503.470109	356820.175234	46.847207
3503.406702	356826.572737	46.852212
3503.371152	356825.433327	46.857217
3503.553611	356816.726942	46.862221
3503.040525	356835.003253	46.867226
3503.596707	356833.057759	46.872231
3503.345042	356837.245630	46.877236
3503.455774	356835.726826	46.882241
3503.419411	356831.406588	46.887245
3503.159335	356833.839899	46.892250
3503.581815	356832.755316	46.897255
3503.387020	356809.399820	46.902260
3503.171798	356798.084297	46.907265
3503.441120	356797.711014	46.912269
3503.490355	356796.074693	46.917274
3503.405839	356797.894955	46.922279
3503.528336	356791.157516	46.927284
3503.582710	356801.277211	46.932289
3503.646159	356799.536852	46.937293
3503.544128	356799.527650	46.942298
3503.726314	356797.539491	46.947303
3503.426073	356781.402346	46.952308
3503.270001	356775.650509	46.957313
3503.213194	356769.526711	46.962317
3503.078314	356763.186226	46.967322
3503.205058	356767.034353	46.972327
3503.350791	356771.108507	46.977332
3503.301001	356760.657491	46.982337
3503.289434	356762.262639	46.987341
3503.134143	356776.130850	46.992346
3503.219721	356767.337981	46.997351
3503.239077	356763.696016	47.002356
3503.496368	356768.312382	47.007361
3503.487877	356767.779438	47.012365
3503.298038	356781.042364	47.017370
3503.262218	356785.984993	47.022375
3503.216325	356777.823656	47.027380
3503.079853	356781.458918	47.032385
3503.192184	356782.560972	47.037389
3503.292504	356785.471711	47.042394
3503.489226	356787.934598	47.047399
3503.451156	356790.612738	47.052404
3503.328110	356789.665294	47.057409
3503.506523	356781.417600	47.062413
3503.548187	356784.948356	47.067418
3503.505470	356782.690380	47.072423
3503.330349	356773.022611	47.077428
3503.317158	356748.722260	47.082433
3503.344997	356748.616183	47.087437
3502.843904	356754.395804	47.092442
3503.056309	356747.593249	47.097447
3503.177751	356761.366819	47.102452
3503.563277	356780.340858	47.107457
3503.172837	356771.012501	47.112461
3503.355858	356760.193859	47.117466
3503.391918	356760.239168	47.122471
3503.222178	356760.698729	47.127476
3502.852342	356759.866643	47.132481
3503.188904	356756.581692	47.137485
3503.420962	356764.128533	47.142490
3503.284926	356764.582765	47.147495
3503.523372	356756.147442	47.152500
3503.455541	356756.641787	47.157505
3503.533468	356752.507055	47.162509
3503.902972	356768.022744	47.167514
3503.625107	356761.475835	47.172519
3503.624902	356772.342147	47.177524
3503.701231	356751.717560	47.182529
3503.591437	356736.364618	47.187533
3503.420941	356729.775283	47.192538
3503.343235	356728.209924	47.197543
3503.198321	356726.986011	47.202548
3503.393022	356722.425651	47.207553
3503.333638	356737.856468	47.212557
3503.367765	356738.309247	47.217562
3503.834772	356747.294914	47.222567
3503.739813	356736.571108	47.227572
3503.250059	356716.341374	47.232577
3503.637204	356698.823144	47.237581
3503.376859	356701.663668	47.242586
3503.594985	356693.129757	47.247591
3503.625651	356698.825315	47.252596
3503.370606	356686.701735	47.257601
3503.425985	356698.449947	47.262605
3503.598881	356708.016521	47.267610
3503.948246	356682.182851	47.272615
3503.539927	356675.987375	47.277620
3503.407987	356659.518210	47.282625
3503.488335	356662.432113	47.287629
3503.349373	356662.276063	47.292634
3503.380259	356653.771747	47.297639
3503.492546	356667.546789	47.302644
3503.714094	356668.326206	47.307649
3503.773855	356662.718369	47.312653
3503.473403	356645.639647	47.317658
3503.679551	356630.669335	47.322663
3503.869178	356631.275665	47.327668
3503.683926	356626.240962	47.332673
3503.765777	356619.942538	47.337677
3503.376598	356619.418881	47.342682
3503.576683	356607.961314	47.347687
3503.180827	356608.100355	47.352692
3503.096752	356602.947863	47.357697
3503.403034	356603.306720	47.362701
3503.155508	356613.830451	47.367706
3503.615370	356601.492036	47.372711
3503.466836	356612.687207	47.377716
3503.302480	356620.118607	47.382721
3503.365063	356610.235092	47.387725
3503.169767	356612.225561	47.392730
3503.267741	356614.907650	47.397735
3503.382159	356612.217660	47.402740
3503.350205	356608.151183	47.407745
3503.700619	356617.918739	47.412749
3503.226480	356627.613069	47.417754
3503.644935	356606.781648	47.422759
3503.668534	356586.623389	47.427764
3503.196990	356591.125967	47.432769
3503.332577	356572.120596	47.437773
3503.219762	356574.581534	47.442778
3503.301292	356571.922189	47.447783
3503.400039	356573.433560	47.452788
3503.245740	356580.125390	47.457793
3503.684658	356579.979771	47.462797
3503.235199	356590.102819	47.467802
3503.769258	356575.029754	47.472807
3503.670149	356584.461220	47.477812
3503.323195	356581.106182	47.482817
3503.760207	356546.657233	47.487821
3503.394197	356543.177967	47.492826
3503.414225	356546.712161	47.497831
3503.358751	356548.655079	47.502836
3503.294643	356549.810480	47.507841
3503.698123	356544.733589	47.512845
3503.133953	356560.982251	47.517850
3503.362033	356549.342110	47.522855
3503.626026	356549.478623	47.527860
3503.045582	356565.170006	47.532865
3503.204365	356546.949839	47.537869
3503.436059	356556.939759	47.542874
3503.748402	356548.747197	47.547879
3503.686239	356533.717484	47.552884
3503.337890	356521.761302	47.557889
3503.337149	356513.898157	47.562893
3503.122130	356518.665560	47.567898
3502.992841	356515.199764	47.572903
3503.294010	356510.698896	47.577908
3503.117135	356513.144517	47.582913
3503.406866	356514.625696	47.587917
3503.600396	356513.729989	47.592922
3503.700104	356518.829352	47.597927
3503.433029	356528.083801	47.602932
3503.244305	356519.486942	47.607937
3504.014483	356510.382213	47.612941
3503.485797	356518.252945	47.617946
3503.163975	356503.925917	47.622951
3503.457711	356495.558153	47.627956
3503.138703	356492.096901	47.632961
3502.981188	356496.727976	47.637965
3503.137253	356495.863639	47.642970
3503.179712	356486.212312	47.647975
3503.065743	356489.793141	47.652980
3503.057367	356484.043369	47.657985
3503.246491	356496.126754	47.662989
3503.027389	356520.947690	47.667994
3503.312360	356525.228881	47.672999
3503.271784	356524.141155	47.678004
3502.844209	356531.995899	47.683009
3503.295980	356536.327063	47.688013
3503.093912	356543.535406	47.693018
3503.174083	356539.782018	47.698023
3503.013469	356547.849032	47.703028
3503.058823	356543.897567	47.708033
3503.434029	356538.163502	47.713037
3503.397315	356545.091225	47.718042
3503.353753	356547.897485	47.723047
3503.400488	356541.222886	47.728052
3503.304901	356549.101485	47.733057
3503.693602	356541.202224	47.738061
3503.374185	356528.274452	47.743066
3503.174360	356505.606702	47.748071
3503.006563	356506.905736	47.753076
3502.874717	356513.619473	47.758081
3503.555453	356507.022771	47.763085
3503.079952	356516.259277	47.768090
3503.355358	356514.230921	47.773095
3503.368090	356518.733287	47.778100
3503.237971	356525.981154	47.783105
3503.334225	356518.662527	47.788109
3503.065152	356514.557187	47.793114
3503.372828	356520.997854	47.798119
3503.436403	356517.806940	47.803124
3503.171331	356529.071449	47.808129
3503.379800	356518.146940	47.813133
3503.457769	356520.883093	47.818138
3503.423431	356522.949909	47.823143
3503.646465	356528.411492	47.828148
3503.293013	356523.556057	47.833153
3503.727488	356523.207558	47.838157
3503.456709	356536.814167	47.843162
3503.226959	356511.580921	47.848167
3503.144724	356496.707057	47.853172
3503.040967	356498.683058	47.858177
3503.213731	356507.817078	47.863181
3503.233692	356533.516335	47.868186
3503.145218	356515.487935	47.873191
3503.348912	356526.296617	47.878196
3503.332598	356531.312531	47.883201
3503.313603	356506.351337	47.888205
3502.936097	356505.164190	47.893210
3503.286075	356512.437949	47.898215
3503.461987	356526.890062	47.903220
3503.347294	356506.982665	47.908225
3503.599396	356491.725121	47.913229
3503.295641	356497.931634	47.918234
3503.365569	356492.678440	47.923239
3503.729852	356501.604048	47.928244
3503.544959	356497.918010	47.933249
3503.410765	356501.883754	47.938253
3503.196359	356504.462548	47.943258
3503.574892	356510.077684	47.948263
3503.550256	356501.225850	47.953268
3503.231523	356493.565662	47.958273
3503.271832	356470.783588	47.963277
3503.455015	356463.502106	47.968282
3503.311126	356468.919912	47.973287
3503.700926	356471.963039	47.978292
3503.116652	356468.874544	47.983297
3503.661549	356461.332294	47.988301
3503.540689	356475.984027	47.993306
3503.608193	356464.318357	47.998311
3503.650502	356471.284493	48.003316
3503.230112	356468.882628	48.008321
3503.506633	356469.577014	48.013325
3503.218768	356457.382223	48.018330
3503.380884	356446.719505	48.023335
3503.613503	356441.440585	48.028340
3503.567259	356452.721412	48.033345
3503.582599	356430.579463	48.038349
3503.271296	356435.616575	48.043354
3503.340575	356435.758424	48.048359
3503.538692	356430.434062	48.053364
3503.345538	356438.633478	48.058369
3503.452300	356424.849419	48.063373
3503.459059	356434.620446	48.068378
3503.360746	356425.194945	48.073383
3503.468547	356412.988487	48.078388
3503.335793	356412.882350	48.083393
3503.541747	356405.139198	48.088397
3503.360134	356412.242535	48.093402
3503.373994	356411.884188	48.098407
3503.469416	356404.565677	48.103412
3503.109826	356418.466285	48.108417
3503.322366	356411.460081	48.113421
3503.206198	356412.700059	48.118426
3503.185403	356423.875077	48.123431
3503.175562	356423.495030	48.128436
3503.145171	356417.061638	48.133441
3503.316881	356413.293769	48.138445
3503.119955	356423.427822	48.143450
3503.181749	356409.065567	48.148455
3503.499215	356417.693217	48.153460
3503.383318	356423.564665	48.158465
3503.568190	356414.985067	48.163469
3503.156575	356417.569596	48.168474
3503.790502	356417.596729	48.173479
3503.145407	356412.736495	48.178484
3503.057206	356432.116383	48.183489
3503.531182	356414.151712	48.188493
3503.345204	356402.653341	48.193498
3503.156848	356390.977208	48.198503
3503.043094	356389.188507	48.203508
3503.143382	356411.057944	48.208513
3503.315365	356406.246669	48.213517
3503.236620	356400.584356	48.218522
3503.284963	356389.583342	48.223527
3503.100183	356392.030219	48.228532
3503.031785	356395.273028	48.233537
3503.496854	356405.302426	48.238541
3503.265431	356403.405089	48.243546
3503.241702	356398.853785	48.248551
3503.557592	356384.654935	48.253556
3503.246577	356394.298073	48.258561
3503.138766	356392.330297	48.263565
3503.166521	356406.220567	48.268570
3503.354501	356395.451958	48.273575
3503.455546	356388.437929	48.278580
3503.365974	356406.113035	48.283585
3503.219456	356397.865753	48.288589
3503.393533	356401.859112	48.293594
3503.521541	356397.487402	48.298599
3503.785964	356392.559719	48.303604
3503.333349	356404.311968	48.308609
3503.539731	356402.854373	48.313613
3503.673690	356410.900287	48.318618
3503.702554	356373.309313	48.323623
3503.353579	356360.411619	48.328628
3502.967669	356370.066602	48.333633
3503.694590	356363.462580	48.338637
3503.124191	356369.609472	48.343642
3503.209089	356371.301174	48.348647
3503.707216	356369.695663	48.353652
3503.005588	356380.520265	48.358657
3503.485806	356365.073931	48.363661
3503.109318	356382.514479	48.368666
3503.339143	356379.577200	48.373671
3503.504361	356370.517192	48.378676
3503.262714	356377.808160	48.383681
3503.488735	356373.700879	48.388685
3503.402030	356376.946584	48.393690
3503.325946	356365.990685	48.398695
3503.618999	356363.068856	48.403700
3503.505491	356342.626801	48.408705
3503.388771	356327.681996	48.413709
3503.175350	356332.550955	48.418714
3503.434334	356329.558168	48.423719
3503.635013	356329.806483	48.428724
3503.251015	356339.715649	48.433729
3503.357538	356335.118299	48.438733
3503.403832	356335.416469	48.443738
3503.235573	356336.155727	48.448743
3503.604349	356339.533008	48.453748
3503.370147	356343.107408	48.458753
3503.592937	356342.003489	48.463757
3503.372295	356324.403082	48.468762
3503.415531	356312.944796	48.473767
3503.557582	356309.359744	48.478772
3503.252998	356312.410867	48.483777
3503.525165	356298.269801	48.488781
3503.770205	356303.168075	48.493786
3503.501425	356313.746124	48.498791
3503.619715	356306.449431	48.503796
3503.502442	356308.732952	48.508801
3503.452903	356289.705846	48.513805
3503.392957	356276.991468	48.518810
3503.357949	356274.401427	48.523815
3503.504213	356267.583816	48.528820
3503.032653	356277.786765	48.533825
3503.418301	356270.727726	48.538829
3503.278602	356274.210847	48.543834
3503.269546	356270.751473	48.548839
3503.386902	356277.476739	48.553844
3503.226267	356278.011209	48.558849
3503.673157	356272.087645	48.563853
3503.434844	356281.261248	48.568858
3503.549617	356283.075469	48.573863
3503.509130	356278.068740	48.578868
3503.190388	356283.030699	48.583873
3503.489142	356275.883607	48.588877
3503.294278	356269.654334	48.593882
3503.300361	356250.822003	48.598887
3503.322931	356252.396323	48.603892
3503.329402	356251.886456	48.608897
3503.551287	356249.001320	48.613901
3503.323412	356246.772593	48.618906
3503.113996	356244.311916	48.623911
3503.558205	356246.862943	48.628916
3503.363551	356247.250103	48.633921
3503.522915	356245.799937	48.638925
3503.655714	356255.601968	48.643930
3503.663502	356249.315207	48.648935
3503.609194	356240.035402	48.653940
3503.680241	356214.805349	48.658945
3503.629095	356213.973766	48.663949
3503.602297	356224.157306	48.668954
3503.660041	356219.084146	48.673959
3503.833735	356212.313088	48.678964
3503.582266	356214.312452	48.683969
3503.458862	356195.627812	48.688973
3503.348977	356198.062858	48.693978
3503.203880	356191.443988	48.698983
3503.836162	356196.484634	48.703988
3503.655238	356188.675373	48.708993
3503.646865	356187.964268	48.713997
3503.509356	356200.735562	48.719002
3503.441066	356177.970525	48.724007
3503.131307	356161.758341	48.729012
3503.377344	356163.882639	48.734017
3503.453057	356154.276887	48.739021
3503.458803	356149.822692	48.744026
3503.276966	356152.854419	48.749031
3503.304865	356156.438292	48.754036
3502.992719	356155.189908	48.759041
3503.279776	356155.679048	48.764045
3503.294496	356167.255676	48.769050
3502.933777	356158.914979	48.774055
3503.295437	356155.422436	48.779060
3503.048359	356169.050846	48.784065
3503.457613	356164.049347	48.789069
3503.514355	356164.905723	48.794074
3503.285386	356159.292581	48.799079
3503.490018	356163.637401	48.804084
3503.409746	356165.329774	48.809089
3503.659777	356159.513664	48.814093
3503.362899	356173.582561	48.819098
3503.145364	356173.337139	48.824103
3503.186793	356169.029993	48.829108
3503.496924	356168.599357	48.834113
3503.368341	356164.064609	48.839117
3503.436340	356144.713490	48.844122
3503.353964	356125.640617	48.849127
3503.435451	356135.654368	48.854132
3503.193461	356130.857617	48.859137
3503.496095	356126.025659	48.864141
3503.509437	356131.494989	48.869146
3503.158845	356135.545869	48.874151
3503.295202	356126.719412	48.879156
3503.109129	356139.320264	48.884161
3503.326273	356127.859891	48.889165
3503.582096	356138.482279	48.894170
3503.781166	356124.149137	48.899175
3503.876716	356128.612997	48.904180
3503.428009	356113.644270	48.909185
3503.467542	356095.188313	48.914189
3503.271601	356093.743419	48.919194
3503.254362	356097.639808	48.924199
3503.508913	356095.691077	48.929204
3503.372382	356098.155788	48.934209
3503.486467	356103.532849	48.939213
3503.488677	356103.176342	48.944218
3503.514297	356095.716133	48.949223
3503.512745	356103.579935	48.954228
3503.185921	356107.550716	48.959233
3503.632261	356096.155893	48.964237
3503.495149	356090.044708	48.969242
3503.325336	356078.009298	48.974247
3503.624777	356067.299341	48.979252
3503.609844	356075.267056	48.984257
3503.785990	356059.105260	48.989261
3503.721299	356076.903787	48.994266
3503.713774	356059.778556	48.999271
3503.552259	356043.364761	49.004276
3503.351826	356036.118417	49.009281
3503.529700	356028.685024	49.014285
3503.375760	356036.725616	49.019290
3503.051892	356028.022799	49.024295
3503.452359	356028.137738	49.029300
3503.504840	356037.341755	49.034305
3503.627860	356032.334601	49.039309
3503.188348	356046.298842	49.044314
3503.199745	356037.695711	49.049319
3503.275890	356033.739337	49.054324
3502.788835	356044.097471	49.059329
3503.335734	356035.409678	49.064333
3502.959208	356042.823810	49.069338
3503.183810	356036.451849	49.074343
3503.409192	356041.505944	49.079348
3502.980842	356042.973423	49.084353
3503.446648	356038.013867	49.089357
3502.999407	356042.258171	49.094362
3503.569412	356035.755259	49.099367
3503.513628	356039.428714	49.104372
3503.157449	356048.162928	49.109377
3503.493787	356045.844992	49.114381
3503.473723	356040.784115	49.119386
3503.380718	356037.185308	49.124391
3503.449912	356026.740776	49.129396
3503.176411	356017.368344	49.134401
3503.322597	356006.886188	49.139405
3503.236050	356014.305376	49.144410
3503.202384	355998.965622	49.149415
3503.643640	355997.165506	49.154420
3503.351973	356002.708518	49.159425
3503.542206	355999.243067	49.164429
3503.241385	356010.462447	49.169434
3503.342336	355999.809305	49.174439
3503.315003	356007.651749	49.179444
3503.368673	356015.684971	49.184449
3503.651661	356006.580832	49.189453
3503.290964	356016.486377	49.194458
3503.194209	356016.679925	49.199463
3503.588722	356010.688267	49.204468
3503.269774	356008.397583	49.209473
3503.362473	355986.294106	49.214477
3503.346348	355984.718988	49.219482
3503.284159	355979.817453	49.224487
3503.531807	355976.979126	49.229492
3503.343629	355974.489629	49.234497
3503.489623	355973.754116	49.239501
3503.344486	355979.172172	49.244506
3503.314975	355975.817804	49.249511
3503.615455	355974.879731	49.254516
3503.294615	355985.542424	49.259521
3503.594347	355976.282943	49.264525
3503.398200	355981.454583	49.269530
3503.374640	355987.362379	49.274535
3503.204592	355989.552465	49.279540
3503.164089	355992.765442	49.284545
3503.526200	355975.352711	49.289549
3502.938925	355967.989379	49.294554
3503.257235	355971.552801	49.299559
3503.296232	355970.299793	49.304564
3503.014068	355981.618023	49.309569
3503.355866	355979.222877	49.314573
3503.319116	355981.162856	49.319578
3503.386740	355952.294136	49.324583
3503.739668	355958.880409	49.329588
3503.618667	355961.139087	49.334593
3503.441650	355956.866458	49.339597
3503.342665	355968.003042	49.344602
3503.292164	355964.931921	49.349607
3503.540589	355960.286654	49.354612
3503.061782	355966.342770	49.359617
3503.284359	355969.972223	49.364621
3503.676757	355961.512428	49.369626
3503.203813	355963.724954	49.374631
3503.405989	355964.227516	49.379636
3503.257336	355964.887334	49.384641
3503.241488	355961.632598	49.389645
3503.316487	355946.173855	49.394650
3503.039400	355940.975465	49.399655
3503.429213	355949.668102	49.404660
3503.228460	355948.580238	49.409665
3503.023574	355934.845316	49.414669
3503.463657	355942.384842	49.419674
3503.157488	355935.231545	49.424679
3503.257293	355926.945243	49.429684
3503.041133	355933.443353	49.434689
3503.360098	355936.014197	49.439693
3503.026707	355949.936240	49.444698
3502.889844	355952.273770	49.449703
3503.373048	355965.710435	49.454708
3503.348853	355977.624084	49.459713
3503.698744	355963.597877	49.464717
3503.713578	355945.374804	49.469722
3503.566239	355943.413259	49.474727
3503.546726	355932.473770	49.479732
3503.391841	355942.575825	49.484737
3503.578224	355931.705576	49.489741
3503.246990	355941.097516	49.494746
3503.273607	355936.538210	49.499751
3503.438054	355931.168223	49.504756
3503.230638	355942.067474	49.509761
3503.462876	355933.582099	49.514765
3502.937947	355926.310697	49.519770
3503.109488	355936.666523	49.524775
3503.500403	355931.082595	49.529780
3503.327034	355926.325872	49.534785
3503.233228	355909.443263	49.539789
3503.383008	355907.383848	49.544794
3503.107380	355911.321102	49.549799
3503.615784	355899.814630	49.554804
3503.453643	355907.042200	49.559809
3503.503900	355898.814623	49.564813
3503.440920	355908.978499	49.569818
3503.438570	355902.922330	49.574823
3503.250699	355901.857877	49.579828
3502.896222	355915.579678	49.584833
3503.146781	355910.221522	49.589837
3503.145757	355913.504607	49.594842
3503.034133	355909.119843	49.599847
3503.265764	355907.225624	49.604852
3503.376351	355910.338376	49.609857
3503.555212	355907.714504	49.614861
3503.379478	355914.104434	49.619866
3503.411903	355915.244588	49.624871
3503.593325	355915.674087	49.629876
3503.533913	355910.975691	49.634881
3503.606192	355893.965027	49.639885
3503.600422	355881.114744	49.644890
3503.493781	355872.962864	49.649895
3503.496522	355869.908768	49.654900
3503.563041	355878.016325	49.659905
3503.576388	355877.174541	49.664909
3503.297473	355882.308379	49.669914
3503.421504	355883.332259	49.674919
3504.009119	355860.234350	49.679924
3503.538218	355863.133657	49.684929
3503.308686	355851.438460	49.689933
3503.661296	355852.833374	49.694938
3503.541457	355858.374684	49.699943
3503.509523	355837.257876	49.704948
3503.357649	355850.362356	49.709953
3503.714653	355832.492317	49.714957
3503.661758	355831.788245	49.719962
3503.545658	355819.057182	49.724967
3503.543707	355804.832074	49.729972
3503.449789	355814.593689	49.734977
3503.277656	355809.226004	49.739981
3503.499762	355802.854408	49.744986
3503.434198	355808.107213	49.749991
3503.633230	355808.330343	49.754996
3503.284234	355809.963420	49.760001
3503.444153	355801.998420	49.765005
3503.442604	355792.837433	49.770010
3503.437664	355783.142569	49.775015
3503.167121	355771.810113	49.780020
3503.010983	355780.029231	49.785025
3503.092348	355785.182465	49.790029
3503.375675	355774.933062	49.795034
3503.138457	355779.296873	49.800039
3503.176993	355766.134178	49.805044
3503.363844	355774.095486	49.810049
3503.433965	355775.484166	49.815053
3503.355135	355783.818303	49.820058
3503.077847	355781.444677	49.825063
3503.175824	355767.101968	49.830068
3502.883936	355779.287019	49.835073
3503.204301	355781.628615	49.840077
3503.319591	355785.809455	49.845082
3503.277016	355795.944679	49.850087
3503.393156	355778.036355	49.855092
3503.061082	355786.181495	49.860097
3503.391578	355770.020653	49.865101
3503.433763	355780.956822	49.870106
3503.336431	355788.326852	49.875111
3503.415816	355782.614022	49.880116
3503.226747	355781.473411	49.885121
3503.239173	355778.875845	49.890125
3503.347850	355786.773166	49.895130
3503.676863	355784.838100	49.900135
3503.659348	355776.544873	49.905140
3503.348211	355792.677433	49.910145
3503.354499	355786.772574	49.915149
3503.268476	355792.766613	49.920154
3503.228283	355791.729707	49.925159
3503.539491	355789.034009	49.930164
3503.341204	355776.646755	49.935169
3503.199243	355755.191032	49.940173
3503.510397	355753.207891	49.945178
3503.280491	355748.383745	49.950183
3503.535348	355753.535003	49.955188
3503.485127	355762.017309	49.960193
3503.370642	355751.881690	49.965197
3503.452855	355754.489972	49.970202
3503.226149	355759.946396	49.975207
3503.719654	355748.951210	49.980212
3503.448585	355752.913203	49.985217
3503.419112	355751.391085	49.990221
3503.528447	355755.140249	49.995226
3503.337866	355739.901568	50.000231
3503.367053	355728.928888	50.005236
3503.437588	355735.992455	50.010241
3503.596962	355730.114284	50.015245
3503.405579	355731.849686	50.020250
3503.255841	355738.566355	50.025255
3503.141659	355736.166941	50.030260
3503.486629	355740.311473	50.035265
3503.398454	355730.655206	50.040269
3503.331341	355744.560656	50.045274
3503.211792	355743.358156	50.050279
3503.232815	355736.560275	50.055284
3503.249794	355737.779219	50.060289
3503.262323	355731.873368	50.065293
3503.509655	355742.751664	50.070298
3503.075201	355749.055276	50.075303
3503.663173	355738.019704	50.080308
3503.464746	355732.147203	50.085313
3503.194453	355715.394224	50.090317
3503.321541	355719.980375	50.095322
3503.061420	355705.465228	50.100327
3502.988490	355704.229910	50.105332
3503.364726	355725.928776	50.110337
3503.428170	355708.435930	50.115341
3503.750529	355697.671376	50.120346
3503.189832	355701.730059	50.125351
3503.846346	355692.744948	50.130356
3503.541672	355705.390106	50.135361
3503.329844	355702.802542	50.140365
3503.553860	355694.165738	50.145370
3503.427679	355699.860758	50.150375
3503.535335	355700.480058	50.155380
3503.180128	355678.116432	50.160385
3503.453233	355676.419234	50.165389
3503.508943	355671.906201	50.170394
3503.446173	355666.623004	50.175399
3503.556295	355672.331565	50.180404
3503.622276	355664.864912	50.185409
3503.508931	355664.348533	50.190413
3503.109802	355669.450501	50.195418
3503.480332	355663.233561	50.200423
3503.711348	355658.489226	50.205428
3503.241446	355656.095149	50.210433
3503.296801	355647.077830	50.215437
3503.484189	355623.966742	50.220442
3503.386105	355623.651536	50.225447
3503.792451	355620.533617	50.230452
3503.397517	355628.103409	50.235457
3503.175391	355624.728573	50.240461
3503.446926	355624.151345	50.245466
3503.553515	355633.321434	50.250471
3503.659712	355616.610694	50.255476
3503.761498	355635.579126	50.260481
3503.572878	355609.804513	50.265485
3503.370381	355600.013606	50.270490
3503.371309	355599.708194	50.275495
3503.590972	355600.818754	50.280500
3503.213245	355592.404307	50.285505
3503.425153	355585.092709	50.290509
3503.139683	355598.269272	50.295514
3503.147738	355597.250182	50.300519
3503.482008	355595.543312	50.305524
3503.278153	355606.722003	50.310529
3503.099266	355609.066192	50.315533
3503.273819	355602.880227	50.320538
3503.035515	355594.392842	50.325543
3503.070841	355605.635513	50.330548
3503.037250	355597.115764	50.335553
3503.407218	355601.205458	50.340557
3503.268500	355607.615022	50.345562
3502.969553	355609.062055	50.350567
3503.348570	355597.550522	50.355572
3503.040599	355621.495259	50.360577
3503.564547	355607.237850	50.365581
3503.585525	355604.918855	50.370586
3503.604795	355612.753993	50.375591
3503.756440	355607.869512	50.380596
3503.884899	355597.771799	50.385601
3503.695861	355569.477851	50.390605
3503.538863	355565.761886	50.395610
3503.277944	355575.778984	50.400615
3503.888760	355557.868722	50.405620
3503.400872	355568.227083	50.410625
3503.219360	355572.658450	50.415629
3503.504349	355568.083712	50.420634
3503.280112	355567.279484	50.425639
3503.131853	355541.498456	50.430644
3503.039233	355556.858543	50.435649
3503.210836	355565.229468	50.440653
3503.221110	355571.564585	50.445658
3502.925856	355570.567998	50.450663
3503.328412	355571.929575	50.455668
3503.081254	355568.660486	50.460673
3503.462712	355571.730435	50.465677
3503.735810	355563.111297	50.470682
3503.369035	355546.297170	50.475687
3503.206336	355530.417811	50.480692
3503.331098	355531.594272	50.485697
3503.470273	355527.322515	50.490701
3503.342255	355531.389151	50.495706
3503.593706	355535.395795	50.500711
3503.593742	355533.919902	50.505716
3503.398068	355535.223368	50.510721
3503.416661	355536.518407	50.515725
3503.546874	355536.370694	50.520730
3503.318001	355506.657904	50.525735
3503.219879	355482.446715	50.530740
3502.980247	355459.581202	50.535745
3503.067130	355424.856015	50.540749
3503.106158	355371.866424	50.545754
3502.561190	355313.014173	50.550759
3502.372044	355250.848199	50.555764
3501.979241	355187.747303	50.560769
3501.629275	355117.106794	50.565773
3501.648227	355034.650627	50.570778
3501.545475	354953.791382	50.575783
3501.341886	354844.801740	50.580788
3500.840156	354743.773552	50.585793
3500.549796	354645.231176	50.590797
3499.938253	354523.377378	50.595802
3499.614809	354411.301010	50.600807
3499.477278	354289.219025	50.605812
3498.885872	354157.665134	50.610817
3498.047580	354033.326575	50.615821
3498.115495	353882.988135	50.620826
3497.192727	353756.804483	50.625831
3496.954568	353609.440298	50.630836
3496.797529	353477.841461	50.635841
3496.195366	353325.418706	50.640845
3495.989167	353177.539261	50.645850
3495.207284	353025.754834	50.650855
3494.891315	352856.361513	50.655860
3493.963018	352694.470322	50.660865
3493.525526	352539.652427	50.665869
3493.403931	352369.488767	50.670874
3492.406001	352202.186253	50.675879
3491.717546	352033.052781	50.680884
3491.327950	351874.382415	50.685889
3490.715616	351700.858434	50.690893
3490.473585	351520.938225	50.695898
3489.537096	351355.124903	50.700903
3489.475659	351162.526111	50.705908
3488.463688	350986.925164	50.710913
3487.715118	350801.763470	50.715917
3487.311705	350628.126640	50.720922
3486.797354	350437.276613	50.725927
3486.201212	350257.535428	50.730932
3485.496849	350060.249597	50.735937
3484.644824	349883.754456	50.740941
3483.851541	349689.484568	50.745946
3483.198256	349504.328846	50.750951
3482.923271	349318.909080	50.755956
3482.129589	349132.196323	50.760961
3481.447579	348952.133566	50.765965
3480.815932	348758.165709	50.770970
3480.537864	348577.427033	50.775975
3479.901210	348381.600683	50.780980
3478.983970	348186.123431	50.785985
3478.549886	347990.314587	50.790989
3477.966839	347787.020270	50.795994
3477.395940	347610.702516	50.800999
3476.589592	347402.275343	50.806004
3475.633300	347221.894056	50.811009
3474.829784	347009.825317	50.816013
3474.596542	346824.848834	50.821018
3473.743033	346644.424012	50.826023
3473.445269	346435.582003	50.831028
3472.468354	346244.892577	50.836033
3471.540828	346041.773752	50.841037
3471.049466	345855.282334	50.846042
3470.513772	345675.465996	50.851047
3469.653925	345471.290895	50.856052
3469.102150	345293.792144	50.861057
3468.490897	345087.311064	50.866061
3467.836687	344906.849308	50.871066
3467.057954	344700.800597	50.876071
3466.528668	344498.071581	50.881076
3465.750550	344306.860760	50.886081
3465.019028	344112.485703	50.891085
3464.549442	343908.803443	50.896090
3463.448234	343721.281698	50.901095
3462.750516	343522.343138	50.906100
3462.219418	343333.737334	50.911105
3461.584901	343142.398252	50.916109
3460.866161	342944.453807	50.921114
3460.128009	342762.064299	50.926119
3459.797601	342559.271801	50.931124
3458.993868	342372.284263	50.936129
3458.589304	342186.073032	50.941133
3458.022811	341994.414115	50.946138
3456.855841	341795.722254	50.951143
3456.299524	341596.220464	50.956148
3455.798414	341406.967569	50.961153
3455.001608	341203.226131	50.966157
3454.104510	341014.085555	50.971162
3453.422572	340819.055732	50.976167
3452.865014	340613.899962	50.981172
3452.129841	340435.270431	50.986177
3451.263653	340247.217213	50.991181
3450.866303	340044.452494	50.996186
3450.189086	339868.765006	51.001191
3449.408377	339670.310751	51.006196
3448.847145	339489.029121	51.011201
3448.296262	339287.660853	51.016205
3447.608248	339101.892522	51.021210
3446.604951	338908.664051	51.026215
3446.129888	338720.340819	51.031220
3445.521358	338519.386546	51.036225
3444.702096	338337.811531	51.041229
3444.144230	338134.455185	51.046234
3443.188507	337951.729686	51.051239
3442.692386	337758.163019	51.056244
3441.987456	337562.795941	51.061249
3441.341455	337387.147654	51.066253
3440.775065	337190.433831	51.071258
3439.629496	337003.051719	51.076263
3439.336325	336819.556434	51.081268
3438.682764	336642.787272	51.086273
3437.814036	336450.548516	51.091277
3437.448751	336258.509625	51.096282
3436.529835	336075.544002	51.101287
3435.686031	335892.820573	51.106292
3435.165897	335706.710599	51.111297
3434.791020	335510.317939	51.116301
3433.708186	335321.215575	51.121306
3432.920242	335149.020567	51.126311
3432.658362	334951.539222	51.131316
3432.093374	334774.191097	51.136321
3430.885005	334581.287930	51.141325
3430.839033	334397.517863	51.146330
3430.161501	334209.264811	51.151335
3429.551522	334006.235133	51.156340
3428.440478	333834.749827	51.161345
3427.970058	333650.230251	51.166349
3427.453513	333446.140400	51.171354
3426.326037	333275.012730	51.176359
3426.010153	333065.518424	51.181364
3425.426079	332897.613449	51.186369
3424.351486	332703.716536	51.191373
3423.886304	332517.589307	51.196378
3423.240550	332329.758985	51.201383
3422.425486	332140.809319	51.206388
3421.961600	331946.431905	51.211393
3421.455809	331763.262312	51.216397
3421.066089	331552.273198	51.221402
3419.725860	331384.204206	51.226407
3419.385443	331181.047461	51.231412
3418.586511	331001.715642	51.236417
3417.966653	330809.345630	51.241421
3417.334390	330624.436519	51.246426
3416.569017	330433.336019	51.251431
3416.085487	330243.565243	51.256436
3415.181986	330068.372045	51.261441
3414.461921	329871.636488	51.266445
3414.158546	329686.087474	51.271450
3413.345764	329504.488358	51.276455
3412.498491	329318.464342	51.281460
3412.048688	329124.866505	51.286465
3411.458337	328933.199856	51.291469
3410.881044	328753.878508	51.296474
3410.154744	328561.595936	51.301479
3409.409879	328377.921164	51.306484
3408.718821	328184.537311	51.311489
3407.889978	327988.908846	51.316493
3407.567471	327810.334259	51.321498
3406.530068	327627.111321	51.326503
3405.903136	327424.779026	51.331508
3405.377851	327244.809456	51.336513
3404.403315	327066.514500	51.341517
3404.234239	326868.385654	51.346522
3403.354014	326682.004064	51.351527
3402.670364	326500.759376	51.356532
3401.862494	326309.324348	51.361537
3401.201203	326116.261682	51.366541
3400.765485	325925.963524	51.371546
3399.748311	325743.675069	51.376551
3399.444880	325550.096168	51.381556
3398.451932	325372.691467	51.386561
3397.876009	325188.880736	51.391565
3397.040493	324999.076461	51.396570
3396.450352	324814.146868	51.401575
3395.819696	324623.214517	51.406580
3395.217128	324437.598605	51.411585
3394.164328	324256.458217	51.416589
3393.750648	324077.533312	51.421594
3392.967580	323897.113318	51.426599
3392.471854	323711.504357	51.431604
3391.671462	323541.601767	51.436609
3391.067430	323350.051234	51.441613
3390.549018	323173.636171	51.446618
3389.551386	322987.697619	51.451623
3388.688594	322807.822602	51.456628
3388.372513	322629.057436	51.461633
3387.867995	322448.615782	51.466637
3387.461683	322259.195769	51.471642
3386.316598	322078.803725	51.476647
3385.852466	321893.236756	51.481652
3385.327576	321710.301556	51.486657
3384.240319	321521.675099	51.491661
3383.667705	321344.933887	51.496666
3383.068908	321160.634300	51.501671
3382.730055	320976.726074	51.506676
3381.633596	320802.078118	51.511681
3381.335985	320620.556061	51.516685
3380.982568	320418.418211	51.521690
3380.002520	320241.230015	51.526695
3379.199576	320050.136596	51.531700
3378.391424	319877.019912	51.536705
3377.650827	319676.494840	51.541709
3377.174768	319500.243994	51.546714
3376.432875	319324.365862	51.551719
3375.807505	319125.603736	51.556724
3375.382500	318953.876084	51.561729
3374.008268	318773.870151	51.566733
3373.875347	318584.042717	51.571738
3373.301780	318416.386122	51.576743
3372.499383	318216.351476	51.581748
3371.934923	318055.058465	51.586753
3371.313033	317861.767603	51.591757
3370.551932	317685.456587	51.596762
3369.614466	317497.409309	51.601767
3369.001509	317310.125157	51.606772
3368.308874	317128.964350	51.611777
3367.388154	316954.612432	51.616781
3366.993798	316766.095904	51.621786
3366.524737	316595.058499	51.626791
3366.024202	316401.185358	51.631796
3365.128601	316232.251836	51.636801
3364.537184	316052.040644	51.641805
3363.495915	315872.740561	51.646810
3362.705264	315693.425986	51.651815
3362.307416	315517.155498	51.656820
3361.629263	315334.894211	51.661825
3361.113206	315157.648723	51.666829
3360.719295	314973.533933	51.671834
3359.709409	314795.220064	51.676839
3358.853896	314614.105944	51.681844
3358.231040	314436.876108	51.686849
3357.449278	314263.668898	51.691853
3357.133668	314072.384839	51.696858
3356.336138	313906.080196	51.701863
3355.746448	313723.954874	51.706868
3355.138622	313542.239529	51.711873
3354.058669	313365.640391	51.716877
3353.782553	313176.869398	51.721882
3353.146853	313012.218387	51.726887
3352.727477	312823.291186	51.731892
3351.761812	312652.376744	51.736897
3350.893452	312465.633449	51.741901
3350.214678	312287.568584	51.746906
3349.483822	312107.831034	51.751911
3349.106742	311927.247849	51.756916
3348.330955	311755.156097	51.761921
3347.415534	311576.796486	51.766925
3346.970946	311399.660806	51.771930
3346.279308	311224.753858	51.776935
3345.902522	311044.372925	51.781940
3345.088285	310880.205353	51.786945
3344.469425	310695.151235	51.791949
3343.640997	310502.134105	51.796954
3342.889829	310333.092055	51.801959
3342.722820	310154.713717	51.806964
3341.839435	309977.619786	51.811969
3340.990042	309803.805155	51.816973
3340.577206	309614.489604	51.821978
3339.881092	309441.388676	51.826983
3338.971750	309259.586799	51.831988
3338.454090	309081.160449	51.836993
3337.524792	308900.023272	51.841997
3336.892875	308717.820193	51.847002
3336.002541	308549.434250	51.852007
3335.471189	308374.777843	51.857012
3335.188772	308203.825172	51.862017
3334.581050	308022.126538	51.867021
3334.229602	307840.565360	51.872026
3333.057636	307661.400095	51.877031
3332.547335	307471.867461	51.882036
3331.796485	307294.901469	51.887041
3330.874264	307115.084766	51.892045
3330.596511	306935.827975	51.897050
3329.312481	306769.131698	51.902055
3328.799152	306580.438581	51.907060
3328.627138	306415.985174	51.912065
3327.615225	306240.536024	51.917069
3327.043064	306063.565556	51.922074
3326.067199	305881.361887	51.927079
3325.698473	305712.176675	51.932084
3324.934516	305536.254464	51.937089
3324.201180	305366.820902	51.942093
3323.850230	305179.526189	51.947098
3322.942983	305008.591753	51.952103
3322.135622	304834.254371	51.957108
3321.496979	304650.416841	51.962113
3320.764987	304477.722361	51.967117
3320.416344	304308.353979	51.972122
3319.394622	304140.950859	51.977127
3319.020804	303965.041338	51.982132
3318.292744	303797.744159	51.987137
3317.764681	303620.126932	51.992141
3316.994933	303434.806075	51.997146
3316.283450	303263.813096	52.002151
3315.516475	303091.300736	52.007156
3315.034413	302915.763584	52.012161
3314.265516	302743.658577	52.017165
3313.384254	302570.603433	52.022170
3312.801128	302405.955678	52.027175
3312.236126	302235.880590	52.032180
3311.638837	302072.558950	52.037185
3310.705144	301888.968331	52.042189
3310.398380	301717.884104	52.047194
3309.724217	301548.946034	52.052199
3309.061844	301368.444228	52.057204
3308.566655	301194.587940	52.062209
3307.785577	301015.199556	52.067213
3307.248689	300842.851992	52.072218
3306.197093	300670.534723	52.077223
3305.552066	300493.365275	52.082228
3305.273901	300313.590960	52.087233
3304.184907	300151.389232	52.092237
3303.548744	299972.766229	52.097242
3302.772826	299796.940989	52.102247
3302.278030	299630.086254	52.107252
3301.801377	299455.257446	52.112257
3301.148020	299284.454664	52.117261
3300.436317	299110.172013	52.122266
3299.663514	298938.470981	52.127271
3299.139745	298759.523317	52.132276
3298.297384	298591.270945	52.137281
3297.306559	298422.659895	52.142285
3297.253241	298241.472615	52.147290
3296.345392	298068.620623	52.152295
3295.335000	297910.173425	52.157300
3294.815169	297729.696091	52.162305
3294.218924	297555.495510	52.167309
3293.947752	297380.912274	52.172314
3292.680612	297211.248727	52.177319
3292.378083	297037.612403	52.182324
3291.578827	296868.944144	52.187329
3290.847100	296703.066420	52.192333
3290.569907	296526.293182	52.197338
3289.901148	296355.642870	52.202343
3288.826106	296173.774781	52.207348
3288.681819	296007.090458	52.212353
3287.713466	295830.986196	52.217357
3287.102610	295660.733594	52.222362
3286.033592	295485.510832	52.227367
3285.478550	295313.772015	52.232372
3284.910464	295144.811038	52.237377
3284.360387	294978.775799	52.242381
3283.556986	294796.965366	52.247386
3283.118957	294643.034524	52.252391
3282.474236	294459.314123	52.257396
3281.753830	294293.992903	52.262401
3281.153087	294126.717113	52.267405
3280.479538	293942.644289	52.272410
3279.479805	293766.364977	52.277415
3278.798501	293600.349428	52.282420
3278.449993	293427.226650	52.287425
3277.554767	293274.487730	52.292429
3277.224963	293089.392065	52.297434
3276.339580	292911.056602	52.302439
3275.800321	292737.505063	52.307444
3275.462828	292572.249338	52.312449
3274.530628	292395.652677	52.317453
3273.880817	292221.608898	52.322458
3272.822434	292061.916903	52.327463
3272.195148	291878.930217	52.332468
3271.523920	291709.040668	52.337473
3270.879448	291555.878963	52.342477
3270.475841	291376.931335	52.347482
3269.551092	291213.015504	52.352487
3268.973238	291040.105558	52.357492
3268.118160	290878.241369	52.362497
3267.481856	290702.666344	52.367501
3266.871165	290532.333491	52.372506
3265.995255	290376.890144	52.377511
3265.743389	290209.047090	52.382516
3264.986812	290037.030668	52.387521
3264.016924	289874.878427	52.392525
3263.889098	289691.505590	52.397530
3262.780562	289530.546601	52.402535
3262.466363	289355.862070	52.407540
3261.449963	289191.857652	52.412545
3260.671148	289027.153394	52.417549
3260.139193	288860.270696	52.422554
3259.565025	288691.917450	52.427559
3258.794708	288531.974062	52.432564
3258.215716	288365.276809	52.437569
3257.141514	288205.228520	52.442573
3257.063637	288032.390462	52.447578
3256.318083	287875.218822	52.452583
3255.723988	287704.372345	52.457588
3254.788493	287540.558000	52.462593
3254.188304	287368.260643	52.467597
3253.914815	287193.593930	52.472602
3253.003832	287036.702746	52.477607
3252.404686	286864.099355	52.482612
3251.651048	286695.315050	52.487617
3250.754363	286536.918771	52.492621
3250.241596	286359.284276	52.497626
3249.454894	286199.724392	52.502631
3249.071849	286023.724635	52.507636
3248.377075	285864.557555	52.512641
3247.475375	285692.408969	52.517645
3247.111795	285524.046322	52.522650
3246.263848	285376.160161	52.527655
3245.961044	285193.729383	52.532660
3245.259030	285030.462754	52.537665
3244.076610	284858.409162	52.542669
3243.614390	284692.939677	52.547674
3243.304705	284529.126894	52.552679
3242.907029	284360.234343	52.557684
3241.640432	284180.502426	52.562689
3241.085455	284013.417403	52.567693
3240.735667	283843.065401	52.572698
3239.710527	283676.232919	52.577703
3239.041146	283510.133609	52.582708
3238.517596	283333.823897	52.587713
3237.603798	283161.879989	52.592717
3237.230935	282993.798017	52.597722
3236.604413	282830.722424	52.602727
3235.878056	282655.361426	52.607732
3235.236726	282483.909027	52.612737
3234.346104	282322.810653	52.617741
3234.375545	282149.087233	52.622746
3232.889398	281989.509206	52.627751
3232.468839	281810.686828	52.632756
3231.757850	281642.275931	52.637761
3231.057184	281475.213175	52.642765
3230.436991	281310.149639	52.647770
3229.787060	281153.036874	52.652775
3229.037689	280974.240821	52.657780
3228.596491	280813.503928	52.662785
3227.512924	280657.987757	52.667789
3227.197102	280487.196447	52.672794
3226.292488	280314.053294	52.677799
3225.635834	280140.743533	52.682804
3225.129714	279982.156080	52.687809
3224.372348	279826.842826	52.692813
3223.634132	279659.505463	52.697818
3222.646604	279499.440521	52.702823
3222.240012	279334.113569	52.707828
3221.834889	279164.049245	52.712833
3220.864919	279009.482611	52.717837
3220.355568	278838.212245	52.722842
3219.482742	278675.480323	52.727847
3219.145066	278510.167812	52.732852
3218.367385	278354.246315	52.737857
3217.760261	278187.728443	52.742861
3216.967216	278023.022753	52.747866
3216.142562	277851.496523	52.752871
3215.418037	277696.203255	52.757876
3214.835899	277534.622225	52.762881
3214.176790	277385.889421	52.767885
3214.007384	277202.136509	52.772890
3212.885128	277046.320342	52.777895
3212.384397	276885.948863	52.782900
3211.985881	276706.561786	52.787905
3210.870226	276545.803679	52.792909
3210.296529	276386.564325	52.797914
3209.628690	276230.345130	52.802919
3209.176239	276064.770420	52.807924
3208.301582	275906.826618	52.812929
3207.564751	275747.613054	52.817933
3207.010265	275576.273151	52.822938
3206.590096	275415.888872	52.827943
3205.394466	275260.033316	52.832948
3205.009974	275088.997603	52.837953
3203.877830	274928.165668	52.842957
3203.525589	274771.794650	52.847962
3202.645427	274605.905580	52.852967
3202.290899	274447.344649	52.857972
3201.795854	274285.978966	52.862977
3200.758656	274141.075242	52.867981
3200.179729	273976.004459	52.872986
3199.755179	273816.639646	52.877991
3199.304894	273655.394253	52.882996
3198.649990	273492.882358	52.888001
3197.866002	273329.117480	52.893005
3197.526962	273144.601891	52.898010
3196.355461	272993.199581	52.903015
3195.844663	272838.763882	52.908020
3195.375432	272673.548500	52.913025
3194.315539	272504.631805	52.918029
3193.834254	272331.905199	52.923034
3193.100747	272179.746022	52.928039
3192.339937	272018.651789	52.933044
3191.336870	271841.652717	52.938049
3191.257067	271693.261358	52.943053
3190.558840	271539.237490	52.948058
3189.707249	271365.423537	52.953063
3189.209065	271205.128321	52.958068
3188.626263	271042.248749	52.963073
3187.257765	270883.848607	52.968077
3186.377641	270726.262611	52.973082
3186.335472	270562.991961	52.978087
3185.570636	270412.467973	52.983092
3184.777108	270258.892355	52.988097
3184.090460	270100.588217	52.993101
3183.878824	269942.565507	52.998106
3183.116762	269779.689073	53.003111
3182.300588	269622.093173	53.008116
3181.695041	269461.662469	53.013121
3180.881226	269311.197386	53.018125
3180.291889	269140.678753	53.023130
3179.641481	268996.045588	53.028135
3179.143784	268830.682593	53.033140
3178.651469	268677.288871	53.038145
3177.543786	268513.728852	53.043149
3177.385580	268342.683787	53.048154
3176.445739	268196.466640	53.053159
3175.584731	268025.762088	53.058164
3174.910981	267876.293922	53.063169
3174.131825	267718.030474	53.068173
3173.517404	267557.907294	53.073178
3173.124459	267397.978333	53.078183
3172.419844	267246.885263	53.083188
3171.879229	267088.125833	53.088193
3171.000978	266922.849089	53.093197
3170.467099	266763.324653	53.098202
3169.677037	266614.715710	53.103207
3168.681735	266449.508588	53.108212
3168.223753	266289.437472	53.113217
3167.457086	266141.869173	53.118221
3167.205892	265978.454589	53.123226
3166.226589	265834.307301	53.128231
3165.605468	265668.684706	53.133236
3164.832680	265514.699627	53.138241
3164.183242	265363.700321	53.143245
3163.783454	265198.475848	53.148250
3162.876290	265048.179610	53.153255
3162.279770	264888.691241	53.158260
3161.736740	264734.924784	53.163265
3160.917387	264582.373641	53.168269
3160.313559	264432.717279	53.173274
3159.531468	264265.847338	53.178279
3159.186367	264109.579418	53.183284
3158.479553	263955.660920	53.188289
3157.544526	263807.407025	53.193293
3157.450392	263641.192549	53.198298
3156.321624	263477.816007	53.203303
3155.671804	263328.727677	53.208308
3155.411324	263170.001859	53.213313
3154.512661	263015.095418	53.218317
3153.738283	262853.573194	53.223322
3153.276482	262701.271902	53.228327
3152.592440	262541.823905	53.233332
3152.074843	262377.256074	53.238337
3150.880483	262225.325609	53.243341
3150.391074	262065.210357	53.248346
3149.561619	261915.514407	53.253351
3148.909912	261750.484241	53.258356
3148.412632	261601.678191	53.263361
3147.573287	261449.386321	53.268365
3147.368013	261295.058640	53.273370
3146.240981	261139.883661	53.278375
3145.511328	260983.601704	53.283380
3145.104701	260826.963103	53.288385
3144.066481	260676.180242	53.293389
3143.570859	260524.267422	53.298394
3142.890633	260367.927052	53.303399
3141.986294	260224.279675	53.308404
3141.735438	260074.289384	53.313409
3140.916585	259924.338125	53.318413
3140.497670	259758.686529	53.323418
3139.707525	259616.167453	53.328423
3138.835907	259450.638626	53.333428
3138.395246	259300.347734	53.338433
3137.519545	259149.820162	53.343437
3137.025983	258987.287919	53.348442
3136.470169	258834.850783	53.353447
3135.499941	258689.279152	53.358452
3135.016819	258531.686257	53.363457
3134.377966	258389.424078	53.368461
3133.594231	258231.598807	53.373466
3132.731115	258086.570874	53.378471
3132.150140	257928.917457	53.383476
3131.508440	257781.562600	53.388481
3130.666534	257640.249832	53.393485
3130.058247	257493.195480	53.398490
3129.793585	257346.570724	53.403495
3129.180653	257192.106291	53.408500
3128.791749	257036.995294	53.413505
3127.947983	256876.531843	53.418509
3127.085062	256724.985103	53.423514
3126.120546	256566.476504	53.428519
3125.674930	256417.487069	53.433524
3125.192290	256264.887244	53.438529
3124.192844	256121.613925	53.443533
3123.444494	255955.533261	53.448538
3122.637762	255813.808622	53.453543
3122.070271	255671.002062	53.458548
3121.641394	255520.558978	53.463553
3120.896598	255371.744963	53.468557
3120.518109	255221.013985	53.473562
3119.789329	255080.627271	53.478567
3118.850954	254932.251687	53.483572
3118.486440	254772.299741	53.488577
3117.782545	254628.165745	53.493581
3117.187146	254478.029928	53.498586
3116.151373	254319.508866	53.503591
3115.776811	254177.309510	53.508596
3115.497353	254026.767503	53.513601
3114.402576	253871.566855	53.518605
3114.100364	253710.256172	53.523610
3113.258748	253568.691456	53.528615
3112.658016	253404.677850	53.533620
3111.942514	253246.132463	53.538625
3110.917692	253098.739716	53.543629
3110.572613	252939.550232	53.548634
3109.765279	252798.872019	53.553639
3109.078687	252641.799656	53.558644
3108.437573	252487.470644	53.563649
3107.597185	252344.735208	53.568653
3107.095513	252187.786778	53.573658
3106.391388	252057.304974	53.578663
3105.797068	251904.369733	53.583668
3105.260777	251745.211575	53.588673
3104.429768	251604.639924	53.593677
3103.559272	251433.412822	53.598682
3102.809452	251291.758980	53.603687
3102.165264	251145.912019	53.608692
3101.583406	251003.034908	53.613697
3100.908223	250863.941734	53.618701
3100.362657	250701.908302	53.623706
3099.772885	250567.895161	53.628711
3099.616348	250409.645885	53.633716
3098.688843	250260.126435	53.638721
3097.734299	250114.507764	53.643725
3097.037458	249951.709555	53.648730
3096.482290	249806.766480	53.653735
3095.764054	249661.314551	53.658740
3094.988784	249513.681677	53.663745
3094.328636	249363.178496	53.668749
3093.910938	249212.306026	53.673754
3093.221839	249058.548035	53.678759
3092.193890	248907.339515	53.683764
3091.944042	248761.050304	53.688769
3091.060922	248625.429921	53.693773
3090.298264	248471.302165	53.698778
3089.409741	248332.576028	53.703783
3089.368007	248180.753751	53.708788
3088.445119	248030.013329	53.713793
3087.383981	247888.309923	53.718797
3087.044105	247740.839042	53.723802
3086.462699	247596.768046	53.728807
3085.756607	247450.603248	53.733812
3084.977658	247300.477438	53.738817
3084.131001	247159.326505	53.743821
3083.727702	247016.857711	53.748826
3083.012289	246868.504906	53.753831
3082.132510	246722.266468	53.758836
3081.621411	246586.690942	53.763841
3080.682167	246440.716864	53.768845
3080.516441	246282.626130	53.773850
3079.791455	246144.410975	53.778855
3078.878473	246009.561719	53.783860
3078.311032	245847.536938	53.788865
3077.668617	245711.779315	53.793869
3076.877677	245565.451626	53.798874
3076.353974	245424.505972	53.803879
3075.809256	245277.706705	53.808884
3075.320685	245131.917331	53.813889
3074.295062	244988.097565	53.818893
3073.853903	244838.965019	53.823898
3073.054740	244696.968705	53.828903
3072.277624	244555.503827	53.833908
3071.982275	244409.124417	53.838913
3071.364792	244262.032193	53.843917
3070.549836	244110.693207	53.848922
3069.749288	243962.662610	53.853927
3069.141494	243810.960133	53.858932
3068.636268	243659.037878	53.863937
3067.627940	243528.051471	53.868941
3067.326618	243368.126662	53.873946
3066.706324	243217.165355	53.878951
3065.790677	243079.594719	53.883956
3065.394253	242932.469022	53.888961
3064.605660	242790.880565	53.893965
3063.888754	242638.687450	53.898970
3063.206895	242506.275314	53.903975
3062.042591	242349.085822	53.908980
3062.158807	242212.422348	53.913985
3061.274839	242075.280710	53.918989
3060.589647	241927.208772	53.923994
3059.905256	241782.956622	53.928999
3059.101008	241637.501300	53.934004
3058.608491	241492.149602	53.939009
3057.696792	241342.408085	53.944013
3057.234602	241196.975547	53.949018
3056.622100	241050.624782	53.954023
3055.878873	240903.836524	53.959028
3055.621483	240757.811882	53.964033
3054.524095	240619.330590	53.969037
3054.218716	240468.755729	53.974042
3053.381917	240319.283759	53.979047
3052.535005	240175.721358	53.984052
3051.932400	240028.861006	53.989057
3051.029298	239884.391137	53.994061
3050.422773	239735.316369	53.999066
3049.772312	239603.819202	54.004071
3049.019568	239452.043252	54.009076
3048.981424	239311.180463	54.014081
3047.761545	239174.961157	54.019085
3047.074880	239022.335000	54.024090
3046.605543	238879.631178	54.029095
3045.796583	238735.173334	54.034100
3045.147906	238594.102509	54.039105
3044.750374	238453.170360	54.044109
3044.109637	238309.501296	54.049114
3043.235117	238168.925115	54.054119
3042.368610	238028.780735	54.059124
3041.792026	237880.263903	54.064129
3041.349499	237737.175351	54.069133
3040.648035	237585.673936	54.074138
3039.969087	237446.544641	54.079143
3039.170760	237295.466388	54.084148
3038.387335	237166.412232	54.089153
3037.627526	237026.710611	54.094157
3037.270472	236879.764630	54.099162
3036.634688	236739.330767	54.104167
3035.782268	236592.361740	54.109172
3035.451636	236449.359052	54.114177
3034.668387	236308.770859	54.119181
3033.948334	236157.860084	54.124186
3033.645412	236017.476353	54.129191
3032.693396	235878.239561	54.134196
3032.146778	235723.966237	54.139201
3030.970644	235593.321049	54.144205
3030.418935	235437.979493	54.149210
3029.725720	235313.649545	54.154215
3029.069568	235168.968639	54.159220
3028.803786	235023.207612	54.164225
3027.647516	234894.546317	54.169229
3027.291743	234746.966574	54.174234
3026.729167	234605.607350	54.179239
3026.017750	234464.297349	54.184244
3025.249391	234323.225730	54.189249
3024.303764	234181.316624	54.194253
3023.976859	234033.351418	54.199258
3023.261351	233902.660973	54.204263
3022.492763	233766.988351	54.209268
3022.337200	233621.313776	54.214273
3021.164364	233473.254151	54.219277
3020.367130	233332.646854	54.224282
3019.795170	233198.649911	54.229287
3018.983940	233049.744342	54.234292
3018.508272	232908.653889	54.239297
3017.818946	232772.257150	54.244301
3017.290480	232620.735745	54.249306
3016.540381	232489.136022	54.254311
3015.609207	232346.157876	54.259316
3015.563013	232196.190413	54.264321
3014.574131	232073.464590	54.269325
3013.819440	231930.637372	54.274330
3012.951864	231792.436954	54.279335
3012.229179	231646.345903	54.284340
3011.644839	231516.096270	54.289345
3011.360924	231380.299386	54.294349
3010.827037	231233.899008	54.299354
3009.961258	231099.289525	54.304359
3009.071802	230959.744305	54.309364
3008.530576	230817.572487	54.314369
3008.035148	230686.393307	54.319373
3007.259896	230548.409291	54.324378
3006.685255	230406.014243	54.329383
3006.122883	230271.408871	54.334388
3005.309695	230123.730453	54.339393
3004.346313	230000.799656	54.344397
3003.788994	229854.787128	54.349402
3003.274846	229716.839433	54.354407
3002.340179	229589.983517	54.359412
3002.099246	229439.338442	54.364417
3001.299156	229309.533509	54.369421
3000.150087	229162.189928	54.374426
2999.881985	229031.995646	54.379431
2999.038093	228898.251683	54.384436
2998.637261	228766.347410	54.389441
2997.634137	228630.872208	54.394445
2997.388121	228493.596899	54.399450
2996.855573	228362.223317	54.404455
2995.820516	228226.804722	54.409460
2995.379275	228087.702269	54.414465
2994.367109	227955.921462	54.419469
2993.992071	227807.566488	54.424474
2993.331880	227674.966550	54.429479
2992.489345	227533.586078	54.434484
2992.089030	227398.424762	54.439489
2991.185974	227272.152826	54.444493
2991.016719	227134.129157	54.449498
2990.473812	226996.521320	54.454503
2989.411904	226851.637614	54.459508
2989.088778	226702.512515	54.464513
2988.299606	226562.576495	54.469517
2987.390521	226426.020540	54.474522
2986.697824	226290.614484	54.479527
2986.103808	226148.853269	54.484532
2985.660172	226002.765610	54.489537
2984.382450	225872.264948	54.494541
2984.010265	225728.432473	54.499546
2983.736273	225594.043353	54.504551
2982.767441	225465.187573	54.509556
2982.425905	225313.852807	54.514561
2981.571263	225179.632672	54.519565
2981.066763	225030.361077	54.524570
2980.177970	224892.022218	54.529575
2979.357482	224758.815792	54.534580
2979.112027	224618.249608	54.539585
2978.101315	224476.939166	54.544589
2977.575873	224331.796754	54.549594
2977.025005	224196.931846	54.554599
2976.214859	224062.528306	54.559604
2975.700838	223918.301405	54.564609
2974.881912	223785.287303	54.569613
2973.962653	223641.697913	54.574618
2973.288236	223506.968307	54.579623
2972.707520	223360.856208	54.584628
2972.392493	223227.164964	54.589633
2971.509555	223104.537077	54.594637
2970.745077	222961.891902	54.599642
2970.189387	222821.199801	54.604647
2969.423760	222682.819839	54.609652
2968.749306	222539.397395	54.614657
2968.138585	222413.672335	54.619661
2967.332583	222267.432467	54.624666
2966.893151	222136.436057	54.629671
2966.388711	222002.242259	54.634676
2965.647876	221861.492111	54.639681
2964.950040	221717.120172	54.644685
2963.782555	221578.742173	54.649690
2963.859389	221445.221111	54.654695
2962.697809	221312.978368	54.659700
2962.186964	221167.801362	54.664705
2961.461203	221038.150597	54.669709
2960.736524	220899.334580	54.674714
2959.973701	220768.098951	54.679719
2959.699921	220643.532785	54.684724
2958.905946	220500.502270	54.689729
2957.816764	220369.115340	54.694733
2957.277377	220240.225682	54.699738
2956.915115	220102.219376	54.704743
2956.224436	219962.775980	54.709748
2955.657788	219832.516571	54.714753
2954.715982	219700.089146	54.719757
2954.245590	219560.840764	54.724762
2953.607327	219423.605001	54.729767
2952.759467	219290.094181	54.734772
2952.317205	219156.570307	54.739777
2951.445827	219018.532082	54.744781
2950.890057	218885.637683	54.749786
2950.541689	218755.485660	54.754791
2949.456971	218614.312409	54.759796
2948.849721	218466.533777	54.764801
2948.237770	218350.362658	54.769805
2947.697888	218204.088669	54.774810
2947.081075	218068.303206	54.779815
2946.149285	217945.907939	54.784820
2945.549810	217797.047489	54.789825
2944.834792	217671.359739	54.794829
2943.936827	217531.635630	54.799834
2943.621999	217395.892745	54.804839
2942.931705	217269.794468	54.809844
2942.048608	217133.925668	54.814849
2941.478649	217002.513585	54.819853
2940.780054	216873.947927	54.824858
2940.104562	216735.488526	54.829863
2939.236212	216609.317800	54.834868
2938.893502	216475.044930	54.839873
2938.360152	216345.932204	54.844877
2937.410429	216211.895968	54.849882
2936.726029	216069.391563	54.854887
2935.895933	215941.153945	54.859892
2935.766456	215810.183528	54.864897
2934.801186	215679.651181	54.869901
2933.951110	215549.699090	54.874906
2933.458328	215418.150514	54.879911
2932.748369	215296.832178	54.884916
2931.995233	215161.863143	54.889921
2931.530316	215032.665685	54.894925
2930.807591	214904.349375	54.899930
2930.372140	214772.563861	54.904935
2929.596441	214638.541351	54.909940
2928.850625	214508.829320	54.914945
2927.975797	214383.809296	54.919949
2927.519526	214245.931198	54.924954
2926.798605	214116.801491	54.929959
2926.170336	213989.757541	54.934964
2925.893547	213857.337745	54.939969
2924.692088	213723.931801	54.944973
2924.155641	213587.060571	54.949978
2923.877362	213461.298685	54.954983
2922.895839	213329.806136	54.959988
2922.235536	213191.084290	54.964993
2921.976927	213067.534747	54.969997
2921.200230	212935.106857	54.975002
2920.503622	212796.811623	54.980007
2919.499285	212676.079255	54.985012
2919.106106	212526.752210	54.990017
2918.347724	212392.960620	54.995021
2917.505672	212271.108698	55.000026
2917.249694	212132.923301	55.005031
2916.377813	212007.958243	55.010036
2915.716185	211863.142748	55.015041
2914.783979	211742.998915	55.020045
2914.169731	211608.613375	55.025050
2913.779655	211477.832788	55.030055
2912.599947	211355.577864	55.035060
2912.664428	211223.211213	55.040065
2911.716856	211098.145367	55.045069
2911.191077	210953.361334	55.050074
2910.317983	210827.164188	55.055079
2909.426555	210695.497287	55.060084
2908.889455	210568.509250	55.065089
2907.945350	210447.020619	55.070093
2907.603937	210309.056345	55.075098
2906.851567	210187.601495	55.080103
2906.034393	210061.435214	55.085108
2905.535467	209924.947669	55.090113
2904.962983	209799.519553	55.095117
2904.324296	209675.260373	55.100122
2903.522253	209555.685561	55.105127
2902.847311	209420.487013	55.110132
2902.506175	209284.637716	55.115137
2901.677521	209161.478750	55.120141
2901.003774	209030.760905	55.125146
2900.671444	208901.656557	55.130151
2899.705808	208774.612765	55.135156
2898.911114	208650.851262	55.140161
2898.397312	208513.109191	55.145165
2897.626170	208381.911790	55.150170
2896.976548	208248.557260	55.155175
2895.973344	208123.264400	55.160180
2895.741594	207996.767835	55.165185
2894.908454	207879.848463	55.170189
2894.247290	207745.809603	55.175194
2893.958626	207614.575644	55.180199
2892.830588	207487.725713	55.185204
2892.592995	207358.800546	55.190209
2891.735844	207236.884511	55.195213
2890.981386	207101.805520	55.200218
2890.386999	206981.439267	55.205223
2889.625663	206851.147257	55.210228
2888.985748	206712.563838	55.215233
2888.369026	206596.567217	55.220237
2887.674178	206465.311010	55.225242
2887.071524	206340.556612	55.230247
2886.213969	206211.783004	55.235252
2885.869107	206084.799322	55.240257
2884.756740	205959.413746	55.245261
2884.344428	205829.234165	55.250266
2883.577899	205694.949349	55.255271
2882.722381	205585.712202	55.260276
2882.357844	205455.933137	55.265281
2881.578728	205336.973963	55.270285
2881.022811	205217.992415	55.275290
2880.434922	205085.347891	55.280295
2879.438501	204958.138941	55.285300
2879.145616	204822.699381	55.290305
2878.446141	204704.810641	55.295309
2877.919780	204583.102258	55.300314
2877.090887	204456.796911	55.305319
2876.035871	204329.954963	55.310324
2875.846501	204192.642444	55.315329
2875.268227	204074.328561	55.320333
2874.440953	203940.579212	55.325338
2874.044944	203814.613971	55.330343
2873.155225	203692.685041	55.335348
2872.617350	203562.110484	55.340353
2871.861610	203436.686640	55.345357
2870.939097	203302.992050	55.350362
2870.327107	203174.949892	55.355367
2869.775487	203052.676099	55.360372
2869.352746	202928.345995	55.365377
2868.567959	202799.288519	55.370381
2867.869733	202674.582643	55.375386
2867.170495	202542.636137	55.380391
2866.530523	202426.282539	55.385396
2865.735208	202284.349281	55.390401
2865.027794	202169.826699	55.395405
2864.399422	202043.444080	55.400410
2863.862216	201922.583038	55.405415
2862.923975	201803.401941	55.410420
2862.594124	201666.334153	55.415425
2861.900997	201544.620550	55.420429
2860.970803	201418.287152	55.425434
2860.435468	201296.498205	55.430439
2859.706521	201171.367893	55.435444
2859.331200	201042.364184	55.440449
2858.282861	200921.319039	55.445453
2857.739299	200788.804858	55.450458
2857.376933	200667.155348	55.455463
2856.709401	200546.852435	55.460468
2856.175978	200420.942071	55.465473
2855.196576	200292.710244	55.470477
2854.449669	200167.241489	55.475482
2853.914139	200040.148879	55.480487
2853.320349	199914.147448	55.485492
2852.750033	199785.826585	55.490497
2851.823852	199663.555993	55.495501
2851.220790	199536.564339	55.500506
2850.709354	199413.757799	55.505511
2849.595156	199287.865696	55.510516
2849.200090	199154.962965	55.515521
2848.635992	199032.305615	55.520525
2847.679332	198912.357537	55.525530
2847.209244	198783.374219	55.530535
2846.460964	198668.216495	55.535540
2845.908598	198541.600926	55.540545
2844.962842	198423.980901	55.545549
2844.231948	198296.299842	55.550554
2843.865145	198174.542148	55.555559
2842.946061	198057.300463	55.560564
2842.594243	197933.543141	55.565569
2841.882682	197811.713634	55.570573
2841.285164	197687.690405	55.575578
2840.425548	197563.161811	55.580583
2840.058692	197442.131131	55.585588
2839.383799	197316.823109	55.590593
2838.711646	197184.859939	55.595597
2838.142729	197066.445241	55.600602
2837.536464	196939.396702	55.605607
2836.579055	196824.479731	55.610612
2836.037844	196680.408732	55.615617
2835.485842	196565.860765	55.620621
2834.262020	196438.198682	55.625626
2833.868641	196315.367944	55.630631
2833.013204	196200.894291	55.635636
2832.633667	196075.911499	55.640641
2831.386264	195968.969672	55.645645
2830.910072	195846.204066	55.650650
2830.638664	195718.571076	55.655655
2829.612299	195602.229903	55.660660
2829.196709	195487.993564	55.665665
2828.547443	195370.982431	55.670669
2827.671106	195249.350466	55.675674
2827.513521	195132.389254	55.680679
2826.509241	195010.218260	55.685684
2826.061625	194879.930478	55.690689
2825.179595	194765.069809	55.695693
2824.503401	194638.725145	55.700698
2823.906287	194514.225981	55.705703
2822.878937	194400.088979	55.710708
2822.643317	194275.329569	55.715713
2821.885607	194160.895926	55.720717
2821.397682	194039.663420	55.725722
2820.894223	193918.141018	55.730727
2820.150893	193786.325137	55.735732
2819.488502	193666.075455	55.740737
2818.531218	193546.165415	55.745741
2818.130915	193428.266869	55.750746
2817.718095	193303.627011	55.755751
2816.788461	193183.229965	55.760756
2815.800247	193058.796366	55.765761
2815.600233	192928.398100	55.770765
2814.299528	192825.975561	55.775770
2814.176912	192696.825285	55.780775
2813.012286	192575.728969	55.785780
2812.385739	192453.275382	55.790785
2811.796708	192337.941301	55.795789
2810.962763	192225.623567	55.800794
2810.470319	192095.006630	55.805799
2809.753276	191987.416760	55.810804
2809.349195	191876.545827	55.815809
2808.587052	191752.652280	55.820813
2807.747372	191639.026301	55.825818
2807.103410	191519.173360	55.830823
2806.534989	191408.393138	55.835828
2805.915651	191283.218569	55.840833
2805.275845	191169.625647	55.845837
2804.495208	191058.116446	55.850842
2804.246293	190931.624526	55.855847
2803.391501	190818.995265	55.860852
2802.508848	190694.042050	55.865857
2801.954911	190573.261135	55.870861
2801.452681	190451.887077	55.875866
2800.910521	190337.097414	55.880871
2800.149592	190221.477517	55.885876
2799.362706	190083.749637	55.890881
2798.737180	189969.890106	55.895885
2797.951926	189854.783864	55.900890
2797.527016	189735.409582	55.905895
2796.595012	189612.566267	55.910900
2795.787205	189497.795252	55.915905
2795.750119	189385.179805	55.920909
2794.708495	189262.303869	55.925914
2794.041043	189139.279930	55.930919
2793.368377	189023.534462	55.935924
2793.120914	188901.780493	55.940929
2792.247309	188774.515374	55.945933
2791.183015	188660.957489	55.950938
2790.853913	188538.772101	55.955943
2790.330728	188424.772853	55.960948
2789.903926	188309.562710	55.965953
2788.989642	188185.664346	55.970957
2788.278185	188066.670453	55.975962
2787.752968	187932.571434	55.980967
2786.510362	187822.173515	55.985972
2786.293441	187699.934383	55.990977
2785.457299	187580.554369	55.995981
2784.797844	187466.808045	56.000986
2784.396824	187339.522873	56.005991
2783.624752	187225.273371	56.010996
2783.069577	187093.967660	56.016001
2782.260155	186973.630824	56.021005
2781.588091	186855.193569	56.026010
2780.883441	186731.596659	56.031015
2780.146810	186625.116158	56.036020
2779.902729	186501.421472	56.041025
2779.184578	186371.339496	56.046029
2778.079485	186255.198706	56.051034
2777.659645	186131.392917	56.056039
2777.084399	186013.616756	56.061044
2776.104595	185890.091144	56.066049
2775.437099	185778.576577	56.071053
2775.061934	185656.049895	56.076058
2774.482561	185540.158421	56.081063
2773.264617	185423.935855	56.086068
2772.871572	185298.423392	56.091073
2772.352507	185182.065305	56.096077
2771.360862	185064.001360	56.101082
2771.070580	184943.269615	56.106087
2770.191993	184829.437350	56.111092
2769.670886	184710.549235	56.116097
2768.724008	184590.507624	56.121101
2767.835316	184473.204927	56.126106
2767.562579	184356.619135	56.131111
2766.704416	184251.995329	56.136116
2766.202619	184126.439754	56.141121
2765.539794	184007.932147	56.146125
2764.673140	183900.524564	56.151130
2764.073162	183777.695134	56.156135
2763.534411	183668.658750	56.161140
2763.116221	183550.584290	56.166145
2762.217480	183433.527622	56.171149
2761.424205	183321.530240	56.176154
2761.081136	183196.829897	56.181159
2760.573724	183087.968071	56.186164
2759.883555	182960.168582	56.191169
2759.159823	182842.487875	56.196173
2758.441799	182721.804459	56.201178
2758.131385	182598.410881	56.206183
2757.215092	182486.066206	56.211188
2756.710447	182360.503369	56.216193
2755.872039	182242.359047	56.221197
2754.930121	182123.112022	56.226202
2754.286388	181988.934952	56.231207
2753.336995	181877.271277	56.236212
2752.823182	181761.862649	56.241217
2752.417121	181646.780713	56.246221
2751.313986	181538.691289	56.251226
2750.740159	181413.320225	56.256231
2750.222288	181307.212104	56.261236
2749.875700	181183.510246	56.266241
2749.127833	181071.778561	56.271245
2748.349013	180953.679185	56.276250
2748.094745	180830.497966	56.281255
2747.108510	180718.321584	56.286260
2746.590364	180595.106517	56.291265
2745.913789	180481.304394	56.296269
2745.062437	180354.682908	56.301274
2744.729530	180234.721330	56.306279
2743.673053	180112.445171	56.311284
2743.133704	179998.190112	56.316289
2742.495290	179889.268014	56.321293
2741.915946	179772.323253	56.326298
2741.681851	179634.895903	56.331303
2740.575452	179525.629110	56.336308
2739.699804	179398.276556	56.341313
2739.402708	179276.722016	56.346317
2738.561331	179160.125723	56.351322
2737.944881	179037.388638	56.356327
2737.016824	178928.056977	56.361332
2736.458148	178809.292676	56.366337
2735.780698	178690.636561	56.371341
2734.791907	178573.709090	56.376346
2734.428500	178462.406687	56.381351
2733.690661	178346.279587	56.386356
2732.959578	178227.442483	56.391361
2732.062454	178118.298820	56.396365
2731.355834	178008.158586	56.401370
2731.186586	177897.221228	56.406375
2730.368115	177781.095749	56.411380
2729.750032	177664.659024	56.416385
2729.370059	177550.283590	56.421389
2728.234254	177436.231712	56.426394
2727.931185	177316.884221	56.431399
2727.493522	177202.824142	56.436404
2726.753821	177076.423760	56.441409
2725.980063	176959.021578	56.446413
2725.203489	176848.399451	56.451418
2724.783323	176714.737831	56.456423
2723.895394	176606.792271	56.461428
2723.288155	176490.268093	56.466433
2722.395952	176383.175969	56.471437
2721.529223	176271.959161	56.476442
2721.156699	176149.471752	56.481447
2720.403573	176039.712966	56.486452
2719.739098	175923.466558	56.491457
2719.015790	175803.630388	56.496461
2718.271263	175694.647010	56.501466
2718.058655	175571.118498	56.506471
2717.077365	175466.853715	56.511476
2716.529258	175347.258222	56.516481
2716.094131	175236.942471	56.521485
2715.065771	175117.550920	56.526490
2714.826875	174998.149121	56.531495
2714.176603	174891.760255	56.536500
2713.316232	174770.371749	56.541505
2712.978624	174652.042237	56.546509
2712.105512	174529.295604	56.551514
2711.446166	174411.615529	56.556519
2710.783000	174303.487843	56.561524
2710.074988	174181.860759	56.566529
2709.472722	174058.538484	56.571533
2708.784951	173949.487217	56.576538
2708.170500	173822.708251	56.581543
2707.580090	173696.472754	56.586548
2706.836600	173587.278683	56.591553
2706.073006	173457.802831	56.596557
2705.535437	173342.370408	56.601562
2705.069971	173214.806685	56.606567
2704.126662	173092.622441	56.611572
2703.317379	172974.130958	56.616577
2702.745619	172869.172136	56.621581
2701.984699	172753.853110	56.626586
2701.746726	172634.979621	56.631591
2701.136535	172504.935703	56.636596
2700.396416	172398.211599	56.641601
2699.405173	172283.553599	56.646605
2698.700515	172161.334417	56.651610
2698.448239	172040.964300	56.656615
2697.682514	171924.821810	56.661620
2696.886280	171799.782247	56.666625
2696.591471	171676.202455	56.671629
2695.430229	171561.052076	56.676634
2694.931236	171430.472672	56.681639
2694.094371	171318.158463	56.686644
2693.570921	171202.717334	56.691649
2692.872515	171092.378454	56.696653
2692.312481	170963.463525	56.701658
2691.532117	170858.911912	56.706663
2690.741720	170736.367392	56.711668
2690.287195	170618.004846	56.716673
2689.775667	170502.067936	56.721677
2688.888126	170394.546039	56.726682
2688.096843	170260.214466	56.731687
2687.561035	170151.009744	56.736692
2687.067341	170023.104782	56.741697
2686.246506	169909.762031	56.746701
2685.447600	169793.898205	56.751706
2685.225466	169660.483177	56.756711
2684.152016	169565.951462	56.761716
2683.654573	169440.617812	56.766721
2683.144871	169315.693447	56.771725
2682.341755	169208.746448	56.776730
2681.892085	169082.452649	56.781735
2680.974493	168966.050592	56.786740
2680.363018	168838.117364	56.791745
2679.869183	168729.266092	56.796749
2679.139394	168611.474696	56.801754
2678.404762	168475.970472	56.806759
2677.696561	168366.200468	56.811764
2677.102440	168242.691785	56.816769
2676.357767	168120.542566	56.821773
2675.551009	168007.279520	56.826778
2675.065553	167888.269043	56.831783
2674.407919	167777.704325	56.836788
2673.704725	167657.877086	56.841793
2672.915424	167541.993143	56.846797
2672.366429	167426.567408	56.851802
2671.747587	167298.589670	56.856807
2671.037683	167190.832476	56.861812
2670.553186	167077.915354	56.866817
2669.833716	166949.585984	56.871821
2669.204359	166831.924092	56.876826
2668.693743	166705.978478	56.881831
2668.009064	166590.093608	56.886836
2667.159541	166465.296055	56.891841
2666.570804	166349.371299	56.896845
2666.021374	166224.628730	56.901850
2665.304114	166103.015776	56.906855
2664.822443	165993.369389	56.911860
2663.772216	165870.182359	56.916865
2663.671957	165741.339419	56.921869
2662.563160	165622.981657	56.926874
2662.257594	165502.068368	56.931879
2661.082578	165371.324387	56.936884
2660.788938	165255.521587	56.941889
2659.861030	165144.346282	56.946893
2659.324920	165022.644594	56.951898
2659.066233	164900.238161	56.956903
2658.422359	164777.727867	56.961908
2657.662433	164658.198989	56.966913
2656.919078	164522.964766	56.971917
2656.283382	164395.597296	56.976922
2655.542131	164275.977699	56.981927
2654.796805	164145.627732	56.986932
2654.208496	164012.239922	56.991937
2653.324855	163892.313553	56.996941
2652.641235	163773.080631	57.001946
2652.203519	163639.505030	57.006951
2651.490633	163525.795758	57.011956
2650.851899	163409.964457	57.016961
2650.369609	163273.167734	57.021965
2649.502452	163160.246928	57.026970
2648.845191	163036.180701	57.031975
2648.310841	162919.406264	57.036980
2647.723043	162785.921154	57.041985
2646.697607	162674.870538	57.046989
2645.942254	162554.788404	57.051994
2645.807875	162421.944801	57.056999
2644.742443	162301.378641	57.062004
2643.885553	162182.356408	57.067009
2643.491968	162055.238497	57.072013
2642.887049	161943.347943	57.077018
2642.235720	161809.723947	57.082023
2641.305237	161700.784554	57.087028
2640.592968	161571.837168	57.092033
2640.127106	161459.061539	57.097037
2639.230259	161331.746229	57.102042
2638.871622	161212.444849	57.107047
2637.973966	161092.631725	57.112052
2637.467707	160974.702201	57.117057
2637.087691	160855.240125	57.122061
2636.432001	160730.151807	57.127066
2635.589111	160606.288679	57.132071
2634.905415	160483.570414	57.137076
2634.364348	160363.296412	57.142081
2633.711095	160228.903124	57.147085
2632.883555	160121.261756	57.152090
2632.503477	159984.385118	57.157095
2631.600676	159868.683398	57.162100
2630.956489	159736.858659	57.167105
2630.582142	159611.971272	57.172109
2629.570043	159488.443999	57.177114
2629.080220	159361.948499	57.182119
2628.287342	159246.294977	57.187124
2627.575017	159128.823806	57.192129
2627.108917	158996.452389	57.197133
2625.885760	158886.563709	57.202138
2625.774572	158757.455070	57.207143
2625.171135	158642.205771	57.212148
2624.400566	158514.079711	57.217153
2624.087433	158391.653288	57.222157
2623.246119	158265.535275	57.227162
2622.802547	158135.375592	57.232167
2621.944328	158011.091825	57.237172
2621.538009	157878.969437	57.242177
2620.916750	157747.555382	57.247181
2619.748186	157612.020681	57.252186
2618.875387	157484.817217	57.257191
2618.803944	157364.377420	57.262196
2617.882147	157251.941805	57.267201
2617.484502	157116.719116	57.272205
2616.596304	156985.947745	57.277210
2616.026982	156849.761745	57.282215
2615.283417	156722.133828	57.287220
2614.753752	156596.620858	57.292225
2614.296590	156468.948500	57.297229
2613.281096	156353.276361	57.302234
2612.477819	156215.973148	57.307239
2611.734531	156091.716242	57.312244
2611.226781	155963.074964	57.317249
2610.794087	155837.168058	57.322253
2609.942303	155716.412785	57.327258
2609.413569	155582.640664	57.332263
2608.670144	155469.890274	57.337268
2607.983346	155337.084841	57.342273
2607.414598	155206.981528	57.347277
2606.480019	155088.377179	57.352282
2605.940884	154954.736300	57.357287
2605.338518	154826.127037	57.362292
2604.865863	154710.717689	57.367297
2604.264458	154578.155936	57.372301
2603.555676	154448.649751	57.377306
2602.979940	154313.517265	57.382311
2602.239393	154187.703416	57.387316
2601.305637	154059.772451	57.392321
2600.861347	153928.332379	57.397325
2599.867640	153807.364918	57.402330
2599.402629	153674.149562	57.407335
2599.047299	153553.170838	57.412340
2598.587140	153417.616897	57.417345
2597.603653	153283.697175	57.422349
2596.657034	153154.653148	57.427354
2596.503842	153024.149246	57.432359
2595.687249	152902.813808	57.437364
2595.035345	152771.093424	57.442369
2594.365442	152642.236331	57.447373
2593.630600	152510.364886	57.452378
2593.056988	152373.968853	57.457383
2592.544739	152244.135029	57.462388
2591.855544	152114.482281	57.467393
2590.976973	151984.440608	57.472397
2590.212655	151850.314005	57.477402
2589.783841	151715.524682	57.482407
2588.981856	151584.646277	57.487412
2588.153856	151459.390459	57.492417
2587.976926	151330.447658	57.497421
2586.961281	151205.324229	57.502426
2586.241759	151065.334340	57.507431
2585.195542	150937.102802	57.512436
2584.809422	150807.763067	57.517441
2584.501341	150682.872680	57.522445
2583.634354	150559.774472	57.527450
2583.143455	150415.811059	57.532455
2582.250999	150296.263939	57.537460
2581.507459	150169.550764	57.542465
2581.205923	150037.887502	57.547469
2580.418394	149932.140571	57.552474
2579.917402	149726.501768	57.557479
2579.196387	149581.955750	57.562484
2578.881160	149454.148022	57.567489
2578.256552	149310.007354	57.572493
2577.341351	149171.149650	57.577498
2576.826085	149039.740380	57.582503
2576.338870	148902.760535	57.587508
2575.429010	148778.366844	57.592513
2574.747693	148629.421413	57.597517
2574.337216	148493.231831	57.602522
2573.290774	148361.744295	57.607527
2572.571299	148222.440277	57.612532
2571.964325	148087.935730	57.617537
2571.338286	147954.159179	57.622541
2570.719789	147818.348578	57.627546
2570.391714	147681.882507	57.632551
2569.473684	147552.411363	57.637556
2568.698200	147411.632838	57.642561
2568.075839	147278.570229	57.647565
2567.415494	147134.216270	57.652570
2566.612028	146997.053256	57.657575
2566.159910	146855.158438	57.662580
2565.498040	146720.642959	57.667585
2565.192800	146591.536128	57.672589
2563.779833	146455.997059	57.677594
2563.317412	146325.975809	57.682599
2562.570148	146181.932264	57.687604
2561.939724	146059.258663	57.692609
2561.310186	145915.845794	57.697613
2560.651629	145806.394051	57.702618
2559.928072	145660.252314	57.707623
2559.333515	145532.072532	57.712628
2558.566506	145398.583296	57.717633
2558.401353	145248.758652	57.722637
2557.212125	145125.427506	57.727642
2556.779690	144995.699297	57.732647
2555.925476	144856.685636	57.737652
2555.334009	144731.990546	57.742657
2555.123392	144583.472477	57.747661
2554.178827	144464.972164	57.752666
2553.679607	144311.291061	57.757671
2552.803022	144184.305189	57.762676
2552.135949	144043.397523	57.767681
2551.726726	143907.316517	57.772685
2550.516831	143776.598378	57.777690
2550.321775	143630.179099	57.782695
2549.392695	143498.286696	57.787700
2548.381315	143356.559943	57.792705
2548.111047	143236.496163	57.797709
2547.442017	143107.982400	57.802714
2546.961326	142974.458225	57.807719
2545.874282	142832.263020	57.812724
2545.015409	142702.307052	57.817729
2544.858281	142572.278536	57.822733
2543.974898	142443.801529	57.827738
2543.601241	142307.696549	57.832743
2542.586405	142177.538811	57.837748
2542.044912	142042.935572	57.842753
2541.903605	141913.974695	57.847757
2540.921322	141779.569545	57.852762
2540.329788	141641.329278	57.857767
2539.842193	141502.043959	57.862772
2539.033209	141379.163118	57.867777
2538.478330	141224.820161	57.872781
2537.490813	141100.266122	57.877786
2536.956500	140948.564183	57.882791
2536.658740	140819.518395	57.887796
2536.126079	140679.710348	57.892801
2535.393169	140535.462222	57.897805
2534.266992	140397.032847	57.902810
2534.055083	140259.310488	57.907815
2533.204657	140123.570403	57.912820
2532.550096	139988.282702	57.917825
2531.980285	139834.088989	57.922829
2530.963661	139701.159677	57.927834
2530.457470	139555.076141	57.932839
2529.647242	139422.915796	57.937844
2529.036331	139284.092257	57.942849
2528.617549	139150.117740	57.947853
2527.712449	139016.563944	57.952858
2527.482826	138863.782418	57.957863
2526.753715	138742.017759	57.962868
2525.972278	138600.060864	57.967873
2525.636986	138447.844537	57.972877
2524.644643	138311.995428	57.977882
2523.847003	138175.214037	57.982887
2523.101735	138026.660330	57.987892
2522.671853	137897.025558	57.992897
2521.931439	137748.637640	57.997901
2521.241467	137619.553497	58.002906
2520.736860	137466.759230	58.007911
2519.875522	137332.685204	58.012916
2519.215837	137199.647000	58.017921
2518.602649	137060.605559	58.022925
2517.978222	136929.214561	58.027930
2517.330626	136789.138104	58.032935
2516.608943	136640.574946	58.037940
2516.033909	136493.170783	58.042945
2515.636378	136360.234580	58.047949
2514.668252	136222.854087	58.052954
2514.560784	136072.100299	58.057959
2513.483877	135935.017890	58.062964
2512.680149	135791.312240	58.067969
2512.266268	135642.502112	58.072973
2511.111048	135510.248847	58.077978
2510.447046	135357.554377	58.082983
2510.011750	135213.678854	58.087988
2509.496987	135087.614274	58.092993
2509.051165	134942.801703	58.097997
2508.052749	134809.485100	58.103002
2507.621580	134654.991655	58.108007
2507.107140	134516.569171	58.113012
2506.176446	134366.996393	58.118017
2505.640112	134229.226623	58.123021
2504.859942	134089.946384	58.128026
2503.708785	133940.385364	58.133031
2503.544550	133813.737265	58.138036
2502.649776	133670.463090	58.143041
2502.080913	133522.577654	58.148045
2501.566971	133387.818944	58.153050
2500.960513	133242.481469	58.158055
2500.445475	133098.756181	58.163060
2499.643309	132956.576034	58.168065
2499.008203	132811.499346	58.173069
2498.490941	132663.025864	58.178074
2497.798722	132529.429984	58.183079
2496.850507	132376.491553	58.188084
2496.309111	132242.707984	58.193089
2495.677203	132094.065112	58.198093
2495.001996	131960.990001	58.203098
2494.653384	131812.227490	58.208103
2493.601997	131669.280359	58.213108
2492.982284	131517.196339	58.218113
2492.429060	131384.472962	58.223117
2491.693031	131234.746048	58.228122
2490.997248	131090.348285	58.233127
2490.503737	130946.605091	58.238132
2489.876555	130793.979986	58.243137
2489.329480	130651.339131	58.248141
2488.391440	130511.237764	58.253146
2487.683181	130354.499918	58.258151
2487.205120	130221.147750	58.263156
2486.825137	130073.047172	58.268161
2486.050827	129923.206311	58.273165
2485.196129	129779.462851	58.278170
2484.548567	129627.114063	58.283175
2483.767864	129481.353639	58.288180
2483.174650	129332.985965	58.293185
2482.556649	129184.026070	58.298189
2481.644056	129044.855200	58.303194
2480.858927	128895.199401	58.308199
2480.614500	128751.897947	58.313204
2479.643804	128620.727149	58.318209
2478.922937	128463.163711	58.323213
2477.969678	128326.860521	58.328218
2477.936215	128181.648907	58.333223
2477.366431	128045.362522	58.338228
2476.674239	127900.663218	58.343233
2476.331664	127750.981566	58.348237
2475.239632	127612.328968	58.353242
2474.812806	127458.344209	58.358247
2474.293932	127309.988314	58.363252
2473.053164	127169.697828	58.368257
2472.729448	127005.844100	58.373261
2471.991111	126872.943021	58.378266
2471.301147	126720.540799	58.383271
2470.628769	126575.896145	58.388276
2469.925796	126433.835128	58.393281
2469.535963	126269.488312	58.398285
2468.761367	126144.025764	58.403290
2467.825304	125993.050865	58.408295
2467.517898	125832.655836	58.413300
2466.838287	125693.376138	58.418305
2466.309921	125538.199179	58.423309
2465.364438	125391.521450	58.428314
2464.750562	125230.835687	58.433319
2464.040880	125098.370510	58.438324
2463.087040	124946.248657	58.443329
2462.536551	124798.978175	58.448333
2461.972543	124669.069880	58.453338
2461.324719	124511.695465	58.458343
2460.457117	124379.652516	58.463348
2459.802559	124228.744439	58.468353
2459.430346	124087.786181	58.473357
2458.450570	123948.753554	58.478362
2457.945062	123794.649679	58.483367
2457.618941	123648.276917	58.488372
2457.081768	123500.884459	58.493377
2456.677796	123344.278226	58.498381
2455.481362	123205.880622	58.503386
2454.813601	123059.387471	58.508391
2454.107838	122905.447451	58.513396
2453.699175	122764.095616	58.518401
2452.878814	122601.833009	58.523405
2452.298772	122468.153997	58.528410
2451.593120	122300.313437	58.533415
2450.968772	122152.485148	58.538420
2449.921956	122006.959421	58.543425
2449.557704	121852.120637	58.548429
2448.666272	121711.295357	58.553434
2448.378504	121563.759830	58.558439
2447.531047	121414.472755	58.563444
2446.772144	121269.210187	58.568449
2446.217330	121117.364363	58.573453
2445.214221	120967.583917	58.578458
2444.528304	120818.680918	58.583463
2444.084425	120665.715483	58.588468
2443.298859	120535.875210	58.593473
2442.878732	120388.824341	58.598477
2442.212996	120243.755825	58.603482
2441.410064	120100.855590	58.608487
2441.026188	119948.284775	58.613492
2440.141093	119809.214469	58.618497
2439.716063	119648.976917	58.623501
2438.945481	119513.362497	58.628506
2438.299757	119362.391921	58.633511
2437.619797	119208.278999	58.638516
2436.972128	119065.270957	58.643521
2436.663581	118913.633772	58.648525
2435.722840	118769.518484	58.653530
2435.317710	118612.921557	58.658535
2434.930534	118451.631631	58.663540
2433.768655	118299.974625	58.668545
2433.196703	118156.692987	58.673549
2432.532552	118004.933417	58.678554
2431.736987	117850.351781	58.683559
2431.178002	117701.192601	58.688564
2430.548304	117551.017172	58.693569
2430.105111	117392.104090	58.698573
2429.229283	117244.121325	58.703578
2428.603779	117091.986507	58.708583
2427.541901	116940.829470	58.713588
2427.301902	116796.036510	58.718593
2426.887240	116625.799732	58.723597
2426.110191	116485.111611	58.728602
2425.507737	116328.712215	58.733607
2424.718017	116175.352105	58.738612
2423.942408	116021.876430	58.743617
2423.115109	115859.828380	58.748621
2422.431423	115720.881522	58.753626
2422.174045	115574.308335	58.758631
2421.239364	115413.689231	58.763636
2420.468145	115259.849330	58.768641
2420.236466	115111.230975	58.773645
2419.033643	114966.194858	58.778650
2418.280889	114807.531033	58.783655
2418.434083	114652.786625	58.788660
2417.155971	114506.203737	58.793665
2416.614252	114345.376795	58.798669
2415.842803	114193.809260	58.803674
2415.391819	114043.670635	58.808679
2414.823535	113893.100884	58.813684
2413.892546	113743.858886	58.818689
2413.738483	113572.059060	58.823693
2412.673327	113427.327324	58.828698
2412.201937	113275.622561	58.833703
2411.669213	113111.831881	58.838708
2410.783852	112964.757820	58.843713
2410.007497	112812.558417	58.848717
2409.062114	112658.305105	58.853722
2408.648810	112500.503249	58.858727
2408.213033	112355.500243	58.863732
2407.450309	112200.801946	58.868737
2407.113802	112048.543823	58.873741
2406.096893	111899.561293	58.878746
2405.270270	111737.939552	58.883751
2404.834454	111590.516765	58.888756
2403.775743	111439.893621	58.893761
2403.518841	111283.927774	58.898765
2403.080815	111134.864412	58.903770
2402.327903	110971.605055	58.908775
2401.567769	110823.045214	58.913780
2400.715703	110667.520308	58.918785
2400.483210	110508.338100	58.923789
2399.464546	110358.978046	58.928794
2398.871980	110209.075407	58.933799
2398.451885	110051.626582	58.938804
2397.713386	109896.577176	58.943809
2396.738732	109736.825954	58.948813
2395.986156	109586.248120	58.953818
2395.789960	109425.842468	58.958823
2394.984305	109276.943854	58.963828
2394.166445	109124.044046	58.968833
2393.804200	108959.600291	58.973837
2393.064841	108809.653358	58.978842
2392.542999	108651.398432	58.983847
2392.085930	108485.634029	58.988852
2390.862326	108333.774363	58.993857
2390.163387	108190.113075	58.998861
2389.424057	108025.158007	59.003866
2388.683122	107877.640970	59.008871
2388.473776	107728.435215	59.013876
2387.510511	107574.673551	59.018881
2387.126166	107415.002622	59.023885
2385.840357	107268.724158	59.028890
2385.455405	107111.231690	59.033895
2385.367710	106953.337801	59.038900
2384.225702	106801.075103	59.043905
2383.627078	106637.978964	59.048909
2383.014184	106497.759386	59.053914
2382.554978	106339.046501	59.058919
2381.890361	106185.335192	59.063924
2381.140654	106021.188591	59.068929
2380.734839	105862.838389	59.073933
2379.768256	105707.953501	59.078938
2379.097289	105545.764520	59.083943
2378.729052	105391.110390	59.088948
2377.743360	105235.831891	59.093953
2377.094158	105070.058042	59.098957
2376.226562	104910.848397	59.103962
2375.972712	104762.251837	59.108967
2375.457259	104613.818229	59.113972
2374.232445	104454.059231	59.118977
2373.881598	104297.455408	59.123981
2373.113109	104144.351069	59.128986
2372.525359	103979.247585	59.133991
2371.731224	103830.019301	59.138996
2370.932779	103675.457253	59.144001
2370.583813	103518.522052	59.149005
2369.811882	103366.292440	59.154010
2368.831922	103214.318838	59.159015
2368.709502	103045.963424	59.164020
2367.748689	102898.112386	59.169025
2367.361853	102744.208046	59.174029
2366.627614	102584.269743	59.179034
2365.776757	102430.441038	59.184039
2365.262810	102278.551852	59.189044
2364.471711	102115.428529	59.194049
2363.963883	101958.027795	59.199053
2363.171974	101810.518430	59.204058
2362.709638	101645.436836	59.209063
2362.171780	101492.306872	59.214068
2361.444179	101338.611716	59.219073
2360.953952	101177.058488	59.224077
2360.077096	101021.448006	59.229082
2359.361558	100860.116666	59.234087
2358.799369	100692.640851	59.239092
2358.172489	100532.585420	59.244097
2357.545156	100371.344986	59.249101
2356.967220	100228.994132	59.254106
2356.344612	100051.859203	59.259111
2355.616294	99884.935711	59.264116
2354.859590	99743.535941	59.269121
2354.245246	99565.769128	59.274125
2353.591376	99406.658196	59.279130
2352.848908	99238.086125	59.284135
2352.239501	99089.721545	59.289140
2351.536318	98930.368014	59.294145
2350.855948	98768.322639	59.299149
2350.023522	98611.116647	59.304154
2349.637060	98453.625365	59.309159
2348.827435	98275.633113	59.314164
2347.835610	98133.164243	59.319169
2347.635340	97977.232364	59.324173
2346.711389	97808.788385	59.329178
2345.886203	97649.406041	59.334183
2345.434963	97490.124075	59.339188
2344.560336	97336.941953	59.344193
2344.418165	97180.460867	59.349197
2343.614176	97032.723994	59.354202
2342.558358	96871.075087	59.359207
2342.212235	96703.740006	59.364212
2341.762577	96553.330743	59.369217
2341.275763	96385.500265	59.374221
2340.266703	96234.883747	59.379226
2339.824394	96063.357525	59.384231
2339.106522	95907.014575	59.389236
2338.409872	95744.765014	59.394241
2337.735926	95577.483912	59.399245
2336.744862	95423.388272	59.404250
2336.134418	95247.994689	59.409255
2335.853509	95094.961915	59.414260
2334.675075	94939.909993	59.419265
2334.056482	94775.632046	59.424269
2333.551708	94613.829503	59.429274
2332.955103	94458.726695	59.434279
2332.268408	94303.943641	59.439284
2331.601788	94143.736518	59.444289
2331.185856	93982.279577	59.449293
2330.189453	93830.738654	59.454298
2329.554540	93671.861580	59.459303
2328.974875	93500.497221	59.464308
2328.427635	93346.852808	59.469313
2327.649655	93183.620109	59.474317
2326.907625	93036.514802	59.479322
2326.229722	92874.714287	59.484327
2326.024740	92706.010631	59.489332
2324.864626	92553.337628	59.494337
2324.216707	92384.231089	59.499341
2323.745312	92226.898305	59.504346
2322.538692	92066.639615	59.509351
2322.396867	91907.202399	59.514356
2321.326730	91756.930150	59.519361
2321.060830	91600.590110	59.524365
2320.150589	91440.441150	59.529370
2319.629360	91288.056031	59.534375
2318.744288	91125.394477	59.539380
2318.360643	90978.188986	59.544385
2318.015937	90809.464926	59.549389
2316.880316	90645.413707	59.554394
2316.241343	90494.682271	59.559399
2315.839171	90341.206976	59.564404
2315.144035	90181.261354	59.569409
2314.542914	90010.047985	59.574413
2313.719096	89844.583829	59.579418
2313.424978	89682.936140	59.584423
2312.500009	89525.834136	59.589428
2311.880863	89367.587929	59.594433
2311.561679	89205.827295	59.599437
2310.369773	89034.087626	59.604442
2310.025725	88878.153495	59.609447
2309.443324	88719.842780	59.614452
2308.423208	88559.548523	59.619457
2307.787704	88399.264196	59.624461
2307.008232	88227.896618	59.629466
2306.516360	88069.855249	59.634471
2305.778758	87914.383537	59.639476
2304.970615	87763.368211	59.644481
2304.872719	87598.008943	59.649485
2304.411426	87434.249081	59.654490
2303.418987	87272.685748	59.659495
2302.808046	87103.335355	59.664500
2302.136487	86935.276467	59.669505
2301.640042	86771.083474	59.674509
2300.835335	86617.406793	59.679514
2300.190683	86443.572397	59.684519
2299.576596	86277.145078	59.689524
2298.603779	86107.149957	59.694529
2298.319913	85940.660207	59.699533
2297.729593	85780.083970	59.704538
2296.763764	85624.506572	59.709543
2296.199975	85459.966666	59.714548
2295.455205	85291.729462	59.719553
2295.105867	85112.039969	59.724557
2294.016433	84965.164875	59.729562
2293.363208	84793.766711	59.734567
2292.875405	84627.161106	59.739572
2292.304723	84476.220085	59.744577
2291.282389	84294.539816	59.749581
2290.622597	84140.610825	59.754586
2289.769662	83978.942578	59.759591
2289.395719	83815.957264	59.764596
2288.681821	83657.844314	59.769601
2287.999449	83500.057145	59.774605
2287.455629	83335.308731	59.779610
2286.683147	83164.811038	59.784615
2285.968227	83002.653022	59.789620
2285.353162	82854.069445	59.794625
2284.792972	82685.418069	59.799629
2284.103612	82522.644909	59.804634
2283.408354	82369.438018	59.809639
2282.723827	82201.228567	59.814644
2281.855763	82025.108167	59.819649
2281.618543	81867.953498	59.824653
2281.150016	81719.063190	59.829658
2280.133122	81549.903981	59.834663
2279.531834	81379.247904	59.839668
2278.675324	81217.506442	59.844673
2278.115752	81061.087107	59.849677
2277.762936	80903.001062	59.854682
2276.958024	80749.899507	59.859687
2276.647998	80562.580603	59.864692
2275.626042	80416.138592	59.869697
2274.949362	80232.993807	59.874701
2274.013528	80075.976149	59.879706
2273.563240	79912.615109	59.884711
2273.188900	79752.823845	59.889716
2272.339658	79588.888580	59.894721
2271.648851	79427.179167	59.899725
2271.097815	79252.888777	59.904730
2270.293971	79091.998393	59.909735
2269.936495	78929.777413	59.914740
2269.120437	78766.800308	59.919745
2268.236292	78588.360664	59.924750
2267.498950	78422.896089	59.929754
2266.837773	78268.788926	59.934759
2266.415578	78097.878064	59.939764
2265.528620	77944.962430	59.944769
2264.788288	77784.680541	59.949774
2264.545344	77620.037499	59.954778
2263.831266	77451.206035	59.959783
2263.184241	77280.686169	59.964788
2262.431119	77131.690338	59.969793
2261.995908	76952.433390	59.974798
2261.170122	76784.930451	59.979802
2260.237315	76635.364804	59.984807
2259.627337	76465.561886	59.989812
2258.821639	76295.119799	59.994817
2258.266677	76126.882353	59.999822
2257.956291	75965.805265	60.004826
2257.180701	75815.321008	60.009831
2256.619609	75645.770640	60.014836
2255.489189	75479.765061	60.019841
2255.319475	75312.214581	60.024846
2254.690158	75156.149158	60.029850
2253.845463	74982.417028	60.034855
2253.689587	74816.382710	60.039860
2252.466652	74650.126201	60.044865
2251.886061	74490.180797	60.049870
2251.739237	74315.431406	60.054874
2250.925378	74143.709992	60.059879
2250.056723	73976.984718	60.064884
2249.328970	73813.412506	60.069889
2248.763901	73627.477485	60.074894
2247.957493	73457.610680	60.079898
2247.306619	73293.694751	60.084903
2246.543518	73116.285077	60.089908
2245.491846	72965.960972	60.094913
2244.674106	72802.062877	60.099918
2244.347532	72642.484715	60.104922
2244.013324	72478.867341	60.109927
2243.025993	72318.490685	60.114932
2242.269209	72149.659740	60.119937
2241.980868	71995.839076	60.124942
2241.084022	71821.369829	60.129946
2240.702369	71665.982836	60.134951
2240.116759	71498.758293	60.139956
2239.101727	71331.090175	60.144961
2238.738449	71160.982655	60.149966
2238.035355	71005.734179	60.154970
2237.247495	70829.109002	60.159975
2236.824450	70663.424006	60.164980
2235.750564	70488.842574	60.169985
2235.634627	70331.016885	60.174990
2234.620783	70174.094993	60.179994
2233.995463	70007.788838	60.184999
2233.425514	69836.243334	60.190004
2232.480836	69673.803795	60.195009
2231.807840	69508.592552	60.200014
2230.853147	69335.129917	60.205018
2230.703204	69189.517970	60.210023
2230.184633	69018.180491	60.215028
2229.254244	68862.845650	60.220033
2228.722319	68687.408890	60.225038
2228.210519	68528.298743	60.230042
2227.508888	68362.823037	60.235047
2226.938408	68187.143545	60.240052
2226.176422	68023.244689	60.245057
2225.572396	67854.711395	60.250062
2225.064006	67683.593026	60.255066
2224.391094	67509.588919	60.260071
2223.797991	67342.622670	60.265076
2222.821595	67175.933989	60.270081
2222.531107	66991.132692	60.275086
2221.597067	66834.560659	60.280090
2220.836560	66658.491321	60.285095
2220.450674	66495.283518	60.290100
2219.529982	66317.890593	60.295105
2218.647077	66163.146117	60.300110
2218.176581	65990.836610	60.305114
2217.460913	65824.884502	60.310119
2217.210751	65653.280833	60.315124
2216.364983	65495.347295	60.320129
2215.485935	65319.818769	60.325134
2214.997261	65150.733480	60.330138
2214.336873	64985.935541	60.335143
2213.506729	64809.355894	60.340148
2213.034802	64639.252930	60.345153
2212.176689	64479.477487	60.350158
2211.535369	64310.154703	60.355162
2211.366702	64145.539287	60.360167
2210.595780	63969.759026	60.365172
2209.927997	63801.853858	60.370177
2209.251315	63623.098404	60.375182
2208.474083	63456.901135	60.380186
2207.362527	63296.121526	60.385191
2207.178991	63107.867554	60.390196
2206.307736	62961.207631	60.395201
2205.497934	62778.862576	60.400206
2205.327923	62612.560536	60.405210
2204.494574	62452.174501	60.410215
2203.902443	62271.427039	60.415220
2203.016663	62100.633618	60.420225
2202.681875	61934.376335	60.425230
2201.893185	61760.648592	60.430234
2200.766778	61601.253321	60.435239
2200.274434	61427.228381	60.440244
2199.427437	61259.497622	60.445249
2198.709432	61090.412005	60.450254
2198.362370	60925.925638	60.455258
2197.518957	60761.522615	60.460263
2196.840539	60593.631767	60.465268
2195.736918	60432.235843	60.470273
2195.572509	60273.079082	60.475278
2195.000468	60110.642457	60.480282
2194.516429	59939.054713	60.485287
2193.569225	59771.584222	60.490292
2193.243176	59610.233464	60.495297
2192.413566	59436.210848	60.500302
2192.020712	59262.516230	60.505306
2191.026289	59108.590859	60.510311
2190.524763	58927.335761	60.515316
2189.592862	58762.939021	60.520321
2189.227433	58595.757125	60.525326
2188.405640	58426.784848	60.530330
2187.605425	58269.429896	60.535335
2187.231496	58093.923225	60.540340
2186.603212	57933.160350	60.545345
2186.057582	57755.117245	60.550350
2185.085366	57590.711963	60.555354
2184.383318	57418.185058	60.560359
2184.072712	57249.708948	60.565364
2182.911943	57083.369485	60.570369
2182.523693	56905.879275	60.575374
2181.793831	56736.211566	60.580378
2180.932368	56580.634038	60.585383
2180.783521	56404.186724	60.590388
2180.060201	56242.095937	60.595393
2179.415211	56074.889393	60.600398
2178.550842	55906.272892	60.605402
2178.049785	55733.761517	60.610407
2177.623784	55560.464513	60.615412
2176.782508	55390.573725	60.620417
2176.291843	55222.920070	60.625422
2175.474492	55041.126622	60.630426
2174.594793	54872.699281	60.635431
2174.086189	54701.046932	60.640436
2173.392204	54541.371573	60.645441
2172.911505	54361.762447	60.650446
2171.914616	54188.122829	60.655450
2171.254837	54022.187341	60.660455
2171.000224	53845.680195	60.665460
2170.090042	53676.702319	60.670465
2169.255342	53514.403406	60.675470
2168.856331	53337.705762	60.680474
2168.001880	53162.300333	60.685479
2167.395079	52997.859326	60.690484
2166.592199	52836.042398	60.695489
2166.033147	52657.288406	60.700494
2165.478652	52490.973682	60.705498
2164.739459	52327.512177	60.710503
2164.193495	52142.667123	60.715508
2163.290684	51977.579933	60.720513
2163.115273	51803.383545	60.725518
2162.200737	51633.615456	60.730522
2161.621219	51475.926438	60.735527
2160.904242	51290.073154	60.740532
2160.012642	51129.873903	60.745537
2159.564303	50941.260653	60.750542
2158.699216	50785.198610	60.755546
2158.280050	50614.152977	60.760551
2157.571104	50436.128200	60.765556
2156.804869	50267.558067	60.770561
2156.078792	50097.413947	60.775566
2155.638914	49924.704581	60.780570
2154.504182	49756.166099	60.785575
2154.177673	49587.611707	60.790580
2153.370931	49423.061123	60.795585
2152.824815	49254.759844	60.800590
2152.330466	49069.786430	60.805594
2151.506193	48916.223947	60.810599
2151.333285	48730.791802	60.815604
2150.305440	48571.291959	60.820609
2149.654165	48388.931900	60.825614
2149.025585	48217.107342	60.830618
2148.296089	48044.114204	60.835623
2147.855148	47871.197180	60.840628
2147.057496	47704.797882	60.845633
2145.975168	47527.478291	60.850638
2145.976152	47345.569571	60.855642
2144.594151	47186.302891	60.860647
2144.497734	47011.002017	60.865652
2143.723524	46844.676698	60.870657
2143.003646	46672.761444	60.875662
2142.336458	46505.226698	60.880666
2141.527010	46330.564470	60.885671
2141.092548	46154.737428	60.890676
2140.155052	45996.334600	60.895681
2139.544830	45820.481858	60.900686
2139.172171	45638.975839	60.905690
2138.212826	45480.021307	60.910695
2137.783837	45302.784962	60.915700
2137.222924	45133.329764	60.920705
2136.346347	44957.521626	60.925710
2135.759811	44787.605752	60.930714
2135.024059	44624.230446	60.935719
2134.445747	44446.855689	60.940724
2133.528650	44273.847216	60.945729
2133.218287	44101.525366	60.950734
2132.562350	43940.114139	60.955738
2131.621937	43766.282646	60.960743
2131.171309	43583.833135	60.965748
2130.800193	43412.514469	60.970753
2129.807682	43234.066648	60.975758
2129.110722	43073.100091	60.980762
2128.694707	42897.473725	60.985767
2128.301969	42722.133225	60.990772
2127.350021	42548.995687	60.995777
2126.866144	42367.060756	61.000782
2126.154821	42186.722840	61.005786
2125.181410	42013.078630	61.010791
2124.402628	41844.537589	61.015796
2123.552303	41665.906323	61.020801
2123.140529	41510.085606	61.025806
2122.511058	41328.627442	61.030810
2121.673310	41161.522247	61.035815
2121.158001	40981.102620	61.040820
2120.463609	40815.707699	61.045825
2119.771262	40645.349692	61.050830
2119.466129	40468.917857	61.055834
2118.610514	40298.363126	61.060839
2118.236050	40106.623241	61.065844
2117.518427	39946.520794	61.070849
2116.837248	39768.002615	61.075854
2116.298691	39595.406304	61.080858
2115.346704	39424.981508	61.085863
2114.715895	39235.644446	61.090868
2113.939282	39077.652596	61.095873
2113.261535	38896.463443	61.100878
2112.978347	38727.349623	61.105882
2111.960507	38548.862865	61.110887
2111.378820	38378.046768	61.115892
2110.638784	38193.356150	61.120897
2109.556337	38032.347942	61.125902
2109.166869	37851.549427	61.130906
2108.475672	37693.903090	61.135911
2108.557517	37503.648705	61.140916
2107.526995	37340.074930	61.145921
2106.453422	37171.279093	61.150926
2105.737596	36989.866627	61.155930
2104.981149	36826.360250	61.160935
2104.797701	36646.468201	61.165940
2103.976672	36491.654579	61.170945
2103.390866	36297.217293	61.175950
2102.507347	36129.226819	61.180954
2101.604261	35955.974677	61.185959
2101.556707	35807.142460	61.190964
2100.931228	35627.943122	61.195969
2100.101853	35462.123974	61.200974
2099.945945	35274.194230	61.205978
2098.686314	35107.449571	61.210983
2098.338750	34923.088152	61.215988
2097.553285	34761.852344	61.220993
2096.988131	34581.698461	61.225998
2096.277730	34394.659969	61.231002
2095.091020	34230.970611	61.236007
2094.558073	34056.285498	61.241012
2093.903342	33890.296207	61.246017
2093.198771	33718.148347	61.251022
2092.762080	33551.016852	61.256026
2092.080131	33367.051254	61.261031
2091.557437	33204.289105	61.266036
2090.667818	33041.322869	61.271041
2089.892894	32863.575516	61.276046
2089.471309	32696.025140	61.281050
2088.460026	32525.390587	61.286055
2088.187899	32344.003997	61.291060
2087.189974	32177.463700	61.296065
2086.595474	32020.040416	61.301070
2086.150166	31836.082721	61.306074
2085.329170	31682.056480	61.311079
2084.922232	31499.200988	61.316084
2084.249746	31332.772434	61.321089
2083.639680	31159.057658	61.326094
2082.783053	30981.114426	61.331098
2081.972177	30821.768131	61.336103
2081.355766	30646.465480	61.341108
2080.665996	30469.476212	61.346113
2080.232487	30306.959182	61.351118
2079.809567	30133.391463	61.356122
2078.575299	29963.471410	61.361127
2078.286494	29786.206275	61.366132
2077.392785	29620.248895	61.371137
2076.706054	29447.422342	61.376142
2075.916957	29274.471670	61.381146
2074.840084	29104.905277	61.386151
2074.495469	28952.371087	61.391156
2074.138719	28777.080445	61.396161
2073.026274	28615.305718	61.401166
2072.572208	28441.596620	61.406170
2071.943073	28290.646235	61.411175
2071.473947	28111.086610	61.416180
2070.423487	27956.424109	61.421185
2069.781470	27786.360114	61.426190
2069.355804	27617.021859	61.431194
2069.004994	27458.943457	61.436199
2068.327680	27290.010318	61.441204
2067.400588	27123.639027	61.446209
2066.656385	26958.199306	61.451214
2066.206732	26784.083115	61.456218
2065.182734	26616.829631	61.461223
2064.937821	26442.321309	61.466228
2064.216245	26279.401346	61.471233
2063.499864	26116.099148	61.476238
2062.883181	25948.856670	61.481242
2062.047599	25784.157480	61.486247
2061.398603	25609.162347	61.491252
2060.777604	25437.881372	61.496257
2060.038548	25280.918960	61.501262
2059.452406	25117.923722	61.506266
2058.538171	24949.639520	61.511271
2057.917878	24785.417907	61.516276
2057.862144	24629.736274	61.521281
2056.809651	24457.778469	61.526286
2056.377474	24275.328180	61.531290
2055.300901	24125.541308	61.536295
2054.617458	23955.431184	61.541300
2053.887558	23790.892871	61.546305
2053.159481	23624.223017	61.551310
2052.713971	23451.403464	61.556314
2052.015801	23301.761700	61.561319
2051.527901	23127.731553	61.566324
2050.535986	22978.765650	61.571329
2049.970728	22811.010067	61.576334
2049.355555	22645.963168	61.581338
2048.254429	22494.835783	61.586343
2047.814522	22322.285825	61.591348
2046.967771	22164.088044	61.596353
2046.544585	22012.334155	61.601358
2045.754665	21857.170415	61.606362
2045.244294	21693.549138	61.611367
2044.929580	21536.385731	61.616372
2043.902740	21374.982388	61.621377
2043.155483	21222.518462	61.626382
2042.589794	21046.752512	61.631386
2041.949412	20905.009561	61.636391
2041.506195	20731.285267	61.641396
2040.677409	20591.439154	61.646401
2039.884833	20414.811847	61.651406
2039.331969	20262.020818	61.656410
2038.632574	20090.059889	61.661415
2038.242175	19936.671474	61.666420
2036.997563	19775.635688	61.671425
2036.466080	19625.371087	61.676430
2036.168863	19465.424863	61.681434
2035.001287	19313.590111	61.686439
2034.113487	19144.823002	61.691444
2033.490223	19009.002413	61.696449
2032.857263	18852.980129	61.701454
2032.190452	18704.004235	61.706458
2031.313180	18562.320444	61.711463
2030.934926	18406.776510	61.716468
2029.996671	18264.026749	61.721473
2028.940591	18132.799936	61.726478
2028.403494	17974.900702	61.731482
2027.467898	17850.587737	61.736487
2026.316958	17709.823080	61.741492
2025.628419	17586.973252	61.746497
2024.516989	17468.627830	61.751502
2023.356200	17350.306143	61.756506
2022.463057	17248.347538	61.761511
2021.752706	17121.191155	61.766516
2021.112557	17027.261137	61.771521
2020.151055	16943.531406	61.776526
2019.525782	16838.912721	61.781530
2018.784050	16726.306135	61.786535
2017.874984	16635.437450	61.791540
2017.045028	16555.572088	61.796545
2016.319683	16459.286499	61.801550
2015.760552	16366.643709	61.806554
2014.690497	16284.819090	61.811559
2014.164683	16197.166057	61.816564
2013.501746	16122.244182	61.821569
2012.360260	16035.895851	61.826574
2011.869509	15958.688643	61.831578
2010.994876	15892.367007	61.836583
2010.348365	15814.392194	61.841588
2009.639858	15741.254926	61.846593
2008.612337	15676.685655	61.851598
2008.330967	15614.360755	61.856602
2007.358690	15550.843057	61.861607
2007.206411	15477.983305	61.866612
2006.532648	15404.569228	61.871617
2005.733533	15334.165651	61.876622
2005.614529	15256.377303	61.881626
2004.729997	15187.050311	61.886631
2003.856752	15119.946272	61.891636
2002.993593	15048.785626	61.896641
2002.413342	14978.268141	61.901646
2001.808390	14905.307142	61.906650
2000.857635	14853.493486	61.911655
2000.519558	14775.558743	61.916660
2000.017552	14714.853558	61.921665
1999.343969	14652.439921	61.926670
1998.492547	14576.625575	61.931674
1998.090872	14517.805716	61.936679
1997.687088	14442.247034	61.941684
1996.682946	14384.145719	61.946689
1995.986237	14316.300785	61.951694
1995.691558	14243.036305	61.956698
1994.770386	14188.210731	61.961703
1994.573071	14106.985066	61.966708
1993.930709	14040.298958	61.971713
1992.887738	13960.704136	61.976718
1992.758893	13896.605727	61.981722
1991.451414	13826.549414	61.986727
1991.108358	13758.069556	61.991732
1990.125730	13694.859710	61.996737
1989.438628	13629.335696	62.001742
1988.970813	13559.881763	62.006746
1988.187604	13497.942610	62.011751
1987.666845	13423.363614	62.016756
1987.190819	13361.376775	62.021761
1986.103026	13293.710890	62.026766
1985.539014	13236.711160	62.031770
1984.931544	13173.920285	62.036775
1984.572325	13098.810691	62.041780
1983.781002	13033.632293	62.046785
1982.923478	12978.435984	62.051790
1982.508000	12906.345495	62.056794
1981.477741	12833.173164	62.061799
1981.324517	12774.264944	62.066804
1980.474855	12705.312894	62.071809
1979.581686	12639.993930	62.076814
1979.247645	12574.104337	62.081818
1978.510047	12514.786612	62.086823
1977.615353	12441.209754	62.091828
1976.544286	12391.929223	62.096833
1975.813606	12325.891195	62.101838
1975.876092	12267.199269	62.106842
1974.845165	12221.905833	62.111847
1974.252538	12161.621320	62.116852
1973.751918	12079.667454	62.121857
1973.219877	12030.373951	62.126862
1972.530074	11961.607832	62.131866
1971.531455	11906.647521	62.136871
1971.271953	11833.747869	62.141876
1970.578668	11773.388750	62.146881
1969.688195	11718.417282	62.151886
1969.483487	11645.971843	62.156890
1968.318517	11582.100212	62.161895
1967.733957	11522.097281	62.166900
1967.076589	11468.390312	62.171905
1966.240481	11410.812919	62.176910
1965.904983	11338.467434	62.181914
1965.173353	11284.551770	62.186919
1964.605764	11221.280029	62.191924
1963.984087	11162.104052	62.196929
1963.148871	11098.846901	62.201934
1963.130256	11030.982929	62.206938
1961.729880	10983.788304	62.211943
1961.357892	10917.544036	62.216948
1960.985179	10846.172206	62.221953
1959.792249	10786.162840	62.226958
1959.325256	10722.487435	62.231962
1958.715539	10660.801611	62.236967
1958.300776	10591.492095	62.241972
1957.524101	10528.035127	62.246977
1956.475374	10471.940163	62.251982
1955.787589	10412.710946	62.256986
1955.313087	10343.619366	62.261991
1954.452640	10291.271799	62.266996
1954.006535	10221.514292	62.272001
1953.359897	10176.570363	62.277006
1952.757529	10113.135996	62.282010
1951.868796	10054.467930	62.287015
1951.379440	9988.597869	62.292020
1950.933641	9924.621468	62.297025
1950.195985	9873.114682	62.302030
1950.022987	9800.637942	62.307034
1948.567920	9746.214986	62.312039
1948.101058	9674.307810	62.317044
1947.680110	9616.293450	62.322049
1946.703412	9549.584703	62.327054
1946.221074	9498.646968	62.332058
1945.252750	9436.083428	62.337063
1944.971867	9366.401092	62.342068
1944.119433	9308.868254	62.347073
1943.523635	9264.816819	62.352078
1942.859404	9190.559457	62.357082
1941.979900	9129.222542	62.362087
1941.318415	9071.990082	62.367092
1940.862592	9017.030880	62.372097
1940.197118	8957.756520	62.377102
1939.674552	8893.698866	62.382106
1939.023679	8832.238118	62.387111
1938.412660	8768.315355	62.392116
1937.776727	8712.253747	62.397121
1936.760659	8647.396230	62.402126
1936.280710	8588.536071	62.407130
1935.256035	8527.395471	62.412135
1935.193612	8475.486901	62.417140
1934.536979	8413.447751	62.422145
1933.756373	8350.564290	62.427150
1933.399530	8288.905653	62.432154
1932.240124	8230.796147	62.437159
1931.919178	8172.044526	62.442164
1930.831797	8100.103772	62.447169
1930.177234	8045.550073	62.452174
1929.752892	7983.429287	62.457178
1929.136787	7931.017259	62.462183
1928.518213	7858.688084	62.467188
1927.668527	7806.496595	62.472193
1927.098677	7741.305141	62.477198
1926.610091	7680.645769	62.482202
1925.327622	7626.013424	62.487207
1925.068073	7559.575209	62.492212
1924.210975	7496.232989	62.497217
1923.122460	7457.865245	62.502222
1923.023580	7392.710198	62.507226
1922.177564	7330.032722	62.512231
1922.004970	7281.920851	62.517236
1921.153446	7217.636253	62.522241
1920.425604	7163.973826	62.527246
1920.021330	7089.556263	62.532250
1918.767293	7044.871211	62.537255
1918.217744	6976.378588	62.542260
1917.653361	6917.913909	62.547265
1917.005669	6860.523662	62.552270
1916.398240	6798.174202	62.557274
1915.751842	6738.210281	62.562279
1915.089770	6669.000177	62.567284
1914.382504	6625.307114	62.572289
1913.786264	6564.080136	62.577294
1913.366705	6517.214857	62.582298
1912.213747	6462.682192	62.587303
1911.633267	6395.024620	62.592308
1911.295754	6339.668011	62.597313
1910.247915	6283.416294	62.602318
1909.942075	6224.904620	62.607322
1909.096887	6169.196986	62.612327
1908.489224	6104.146496	62.617332
1907.971334	6060.602511	62.622337
1907.060151	6000.308148	62.627342
1907.052408	5928.464041	62.632346
1906.193347	5876.373904	62.637351
1905.435467	5811.694030	62.642356
1904.699872	5743.142771	62.647361
1903.728521	5685.016533	62.652366
1903.348468	5641.226312	62.657370
1902.486582	5574.775068	62.662375
1901.763266	5525.621683	62.667380
1901.129643	5469.450856	62.672385
1900.359153	5413.963736	62.677390
1899.815727	5357.485598	62.682394
1898.908746	5302.119162	62.687399
1898.142096	5243.322491	62.692404
1897.711893	5186.516266	62.697409
1896.959189	5134.616933	62.702414
1896.388593	5075.126477	62.707418
1895.749076	5019.833003	62.712423
1894.905080	4965.574676	62.717428
1894.419934	4907.364057	62.722433
1893.567383	4860.477333	62.727438
1893.338472	4791.305039	62.732442
1892.393289	4749.688616	62.737447
1891.679194	4699.101057	62.742452
1891.562576	4640.329781	62.747457
1890.753322	4596.348949	62.752462
1889.949978	4523.499869	62.757466
1889.230860	4482.412236	62.762471
1888.578958	4422.282700	62.767476
1888.011693	4359.048279	62.772481
1887.117822	4311.334637	62.777486
1886.523046	4251.197518	62.782490
1885.883228	4201.415383	62.787495
1885.292757	4145.347646	62.792500
1884.589348	4082.987019	62.797505
1883.620706	4036.547244	62.802510
1883.465167	3973.888728	62.807514
1882.619974	3926.544807	62.812519
1882.190983	3855.533994	62.817524
1881.749896	3807.832909	62.822529
1880.878482	3756.661565	62.827534
1880.143033	3686.859561	62.832538
1879.466022	3632.476328	62.837543
1878.466421	3584.449023	62.842548
1877.891703	3528.218678	62.847553
1877.373922	3466.024418	62.852558
1876.450325	3416.153567	62.857562
1875.628155	3367.609054	62.862567
1874.929861	3306.293502	62.867572
1874.630148	3263.533867	62.872577
1873.870770	3207.012309	62.877582
1873.515952	3144.421303	62.882586
1872.685358	3094.353032	62.887591
1872.005429	3036.981991	62.892596
1871.553495	2995.809573	62.897601
1871.337568	2941.267371	62.902606
1870.337158	2881.490482	62.907610
1869.600943	2827.879075	62.912615
1869.104637	2766.188301	62.917620
1868.485100	2716.932414	62.922625
1867.309392	2666.350241	62.927630
1866.980727	2595.906856	62.932634
1866.393131	2540.595549	62.937639
1865.206538	2482.261449	62.942644
1864.819877	2431.233061	62.947649
1864.129908	2376.067173	62.952654
1863.585117	2316.915790	62.957658
1862.443169	2268.775835	62.962663
1862.277981	2212.693705	62.967668
1861.430654	2157.589114	62.972673
1860.687594	2107.582089	62.977678
1860.000715	2062.083263	62.982682
1859.367046	2008.788206	62.987687
1858.593132	1953.265829	62.992692
1857.907600	1902.008382	62.997697
1857.086772	1851.610050	63.002702
1856.767418	1803.199871	63.007706
1855.695548	1756.641798	63.012711
1854.967180	1708.696676	63.017716
1854.535129	1650.560736	63.022721
1853.728254	1618.262202	63.027726
1853.666103	1559.806880	63.032730
1852.784137	1513.705965	63.037735
1852.210114	1453.487942	63.042740
1851.525802	1409.146751	63.047745
1850.760444	1356.914284	63.052750
1850.386681	1307.573668	63.057754
1849.353937	1257.200796	63.062759
1848.796283	1208.924265	63.067764
1847.985489	1157.100303	63.072769
1847.236435	1111.313108	63.077774
1846.785299	1063.466452	63.082778
1845.896959	1015.269883	63.087783
1845.103682	969.915956	63.092788
1844.458333	925.718296	63.097793
1843.747128	872.400289	63.102798
1843.191243	823.345713	63.107802
1842.335649	789.670568	63.112807
1841.891656	735.381777	63.117812
1841.502253	692.975875	63.122817
1840.669201	651.920273	63.127822
1839.779547	605.778523	63.132826
1839.079729	551.426961	63.137831
1838.438237	503.918310	63.142836
1838.074784	470.749244	63.147841
1837.208845	434.750532	63.152846
1836.667980	386.007291	63.157850
1835.622097	346.993828	63.162855
1834.948948	303.296071	63.167860
1834.287927	255.539023	63.172865
1833.423787	231.787141	63.177870
1832.931261	186.365836	63.182874
1832.323042	153.827717	63.187879
1831.477234	109.787381	63.192884
1831.282113	74.236553	63.197889
1829.957627	47.347442	63.202894
1829.337998	-4.594178	63.207898
1828.319774	-15.735756	63.212903
1827.586912	-54.774181	63.217908
1825.601846	-42.709234	63.222913
1821.033427	48.187969	63.227918
1821.413339	38.637803	63.232922
1821.900455	40.257341	63.237927
1822.280964	32.295051	63.242932
1822.864366	23.676084	63.247937
1822.438352	21.895691	63.252942
1821.078500	29.428681	63.257946
1819.429357	42.244590	63.262951
1819.078797	44.995343	63.267956
1818.613593	39.767700	63.272961
1817.810587	43.623187	63.277966
1818.193503	55.018883	63.282970
1817.641864	50.095116	63.287975
1816.219205	53.930735	63.292980
1815.520529	49.057126	63.297985
1815.089958	53.591478	63.302990
1814.377474	47.248788	63.307994
1813.500886	52.502083	63.312999
1812.807368	49.165162	63.318004
1812.320453	48.867289	63.323009
1811.231736	51.393069	63.328014
1811.361562	51.150221	63.333018
1810.997250	54.858779	63.338023
1810.010760	56.810094	63.343028
1809.431430	53.450309	63.348033
1808.658960	60.268734	63.353038
1807.831005	60.326213	63.358042
1807.367429	56.419774	63.363047
1806.570282	62.693349	63.368052
1806.295405	47.877712	63.373057
1805.001395	61.651215	63.378062
1804.514434	56.485370	63.383066
1803.986028	60.612644	63.388071
1803.096584	62.422396	63.393076
1802.363996	54.903356	63.398081
1801.612823	67.461580	63.403086
1801.256603	59.570538	63.408090
1800.642874	59.236037	63.413095
1799.954121	63.086005	63.418100
1799.375125	61.148558	63.423105
1798.433918	60.556984	63.428110
1798.073164	58.923920	63.433114
1796.999619	54.805272	63.438119
1797.148260	65.227363	63.443124
1796.833195	63.429350	63.448129
1795.271624	66.539578	63.453134
1794.649511	55.931137	63.458138
1793.865721	58.249231	63.463143
1793.475259	54.990341	63.468148
1792.989292	48.378301	63.473153
1792.285606	59.979668	63.478158
1791.676428	49.077447	63.483162
1790.811217	50.990585	63.488167
1790.322628	48.367013	63.493172
1789.709460	48.499196	63.498177
1788.669041	55.248214	63.503182
1788.520738	48.394896	63.508186
1787.626938	51.976235	63.513191
1786.852136	50.688044	63.518196
1786.359243	53.362059	63.523201
1785.510786	57.932817	63.528206
1785.051053	50.182800	63.533210
1784.734424	56.392681	63.538215
1783.858049	54.136618	63.543220
1783.460853	45.570862	63.548225
1782.583505	54.753991	63.553230
1781.279077	47.316315	63.558234
1780.849303	52.044505	63.563239
1780.581995	53.831155	63.568244
1779.714403	47.636110	63.573249
1778.362121	62.983189	63.578254
1778.693418	52.276960	63.583258
1778.505336	54.082566	63.588263
1776.861622	47.602355	63.593268
1776.091100	44.895831	63.598273
1775.555922	58.200327	63.603278
1774.803195	52.179426	63.608282
1774.126845	58.574168	63.613287
1774.128587	52.681025	63.618292
1773.896387	54.785370	63.623297
1772.868163	61.272265	63.628302
1772.482450	51.528295	63.633306
1771.433883	59.619003	63.638311
1770.280337	56.976462	63.643316
1769.442284	52.771543	63.648321
1768.693149	69.967196	63.653326
1768.695905	51.964653	63.658330
1767.846344	59.612178	63.663335
1767.108901	64.704623	63.668340
1766.626229	53.862739	63.673345
1765.523369	52.850580	63.678350
1765.023567	54.287807	63.683354
1764.385502	63.076558	63.688359
1764.024504	62.569465	63.693364
1763.438335	53.065487	63.698369
1762.929524	59.457277	63.703374
1762.130056	55.320348	63.708378
1761.557852	54.523529	63.713383
1761.250098	62.916050	63.718388
1760.534282	50.840193	63.723393
1759.093275	65.310409	63.728398
1758.439615	56.099420	63.733402
1757.961833	51.577094	63.738407
1757.060916	60.636245	63.743412
1756.746233	55.908245	63.748417
1756.061724	61.113707	63.753422
1755.731931	61.867933	63.758426
1755.539681	55.731214	63.763431
1754.414486	61.326783	63.768436
1753.613381	57.256346	63.773441
1752.499754	60.274955	63.778446
1752.081543	48.236992	63.783450
1751.264338	52.411716	63.788455
1750.909220	56.106205	63.793460
1749.994031	50.164731	63.798465
1749.551674	58.554974	63.803470
1749.253669	49.104583	63.808474
1747.784792	55.603123	63.813479
1746.859483	56.321047	63.818484
1746.897536	50.759602	63.823489
1746.115135	54.484107	63.828494
1745.513335	58.828047	63.833498
1744.650412	53.972662	63.838503
1744.315530	55.016275	63.843508
1743.848955	52.863872	63.848513
1743.218172	58.847690	63.853518
1742.686615	51.306206	63.858522
1741.624980	59.630807	63.863527
1740.483484	67.706327	63.868532
1739.953514	55.910036	63.873537
1739.287432	58.193680	63.878542
1738.578428	60.220795	63.883546
1738.300331	53.602559	63.888551
1737.702429	58.308574	63.893556
1737.516279	47.941572	63.898561
1737.128612	56.852976	63.903566
1736.096453	47.320500	63.908570
1735.016601	50.363710	63.913575
1734.162992	56.990037	63.918580
1733.918290	45.801295	63.923585
1732.902556	56.189111	63.928590
1732.851548	58.710951	63.933594
1731.587880	50.531980	63.938599
1730.695573	54.884217	63.943604
1730.038949	47.878259	63.948609
1729.278609	58.736438	63.953614
1728.621577	46.140337	63.958618
1728.667147	59.652213	63.963623
1728.509464	54.050895	63.968628
1727.760836	57.125078	63.973633
1727.027455	51.405468	63.978638
1725.603369	60.651799	63.983642
1724.827918	51.537439	63.988647
1723.863432	44.689190	63.993652
1723.844831	52.209470	63.998657
1723.173831	51.489852	64.003662
1722.830315	47.660558	64.008666
1722.325768	52.785402	64.013671
1721.342541	63.166486	64.018676
1720.721129	50.752381	64.023681
1719.686841	55.199711	64.028686
1719.412060	48.587261	64.033690
1719.012272	56.664821	64.038695
1717.483512	56.133484	64.043700
1716.829400	52.875486	64.048705
1715.995141	58.949974	64.053710
1715.665905	49.055126	64.058714
1714.954814	51.315963	64.063719
1714.393436	53.059442	64.068724
1714.422779	53.844937	64.073729
1713.643674	55.334421	64.078734
1713.137861	52.480216	64.083738
1712.114396	58.020218	64.088743
1711.072723	55.721052	64.093748
1710.639066	54.221005	64.098753
1710.021300	56.872291	64.103758
1709.495548	56.269952	64.108762
1709.037799	50.246375	64.113767
1707.615903	57.693091	64.118772
1707.181002	50.632998	64.123777
1706.375530	51.722979	64.128782
1705.973575	51.947787	64.133786
1705.438881	58.078772	64.138791
1705.224783	57.173045	64.143796
1704.876976	51.830585	64.148801
1703.272239	52.255904	64.153806
1702.671051	49.110928	64.158810
1702.140681	50.573522	64.163815
1701.247435	58.496079	64.168820
1701.154125	49.904148	64.173825
1699.619843	58.655492	64.178830
1699.144971	47.541164	64.183834
1698.620929	58.708738	64.188839
1697.937487	49.046773	64.193844
1697.808717	50.669500	64.198849
1697.128467	56.692721	64.203854
1696.465358	53.535504	64.208858
1695.293591	50.835971	64.213863
1694.640979	52.923523	64.218868
1694.493891	51.843154	64.223873
1693.628938	54.891668	64.228878
1693.256828	58.440631	64.233882
1691.826462	51.609627	64.238887
1691.010086	53.190192	64.243892
1690.620189	55.105129	64.248897
1689.729605	56.617059	64.253902
1689.448986	56.455172	64.258906
1689.372487	53.487047	64.263911
1688.847566	64.175380	64.268916
1688.468920	55.890542	64.273921
1686.843452	62.522797	64.278926
1686.501745	56.089712	64.283930
1685.617515	59.202793	64.288935
1684.435734	62.489293	64.293940
1684.197062	47.272130	64.298945
1683.136926	57.720630	64.303950
1682.806838	53.588016	64.308954
1682.338016	50.177595	64.313959
1681.796420	64.413508	64.318964
1681.736574	53.625909	64.323969
1680.513384	50.083011	64.328974
1679.741289	58.642331	64.333978
1679.135287	48.646379	64.338983
1678.148134	60.458369	64.343988
1677.911767	51.089662	64.348993
1676.296646	66.472225	64.353998
1676.024046	55.444036	64.359002
1675.563745	52.831765	64.364007
1674.599191	61.519429	64.369012
1674.607012	57.605946	64.374017
1673.931051	59.787097	64.379022
1673.786671	55.880446	64.384026
1672.745329	54.133168	64.389031
1671.782277	58.707969	64.394036
1671.494978	46.344889	64.399041
1670.332337	50.024160	64.404046
1669.366664	44.921782	64.409050
1668.649388	50.070963	64.414055
1668.123990	56.004937	64.419060
1667.620654	38.458133	64.424065
1667.501395	51.816406	64.429070
1666.879482	59.173908	64.434074
1666.378528	44.860996	64.439079
1665.139287	61.491120	64.444084
1664.799097	47.245707	64.449089
1664.037508	54.311587	64.454094
1663.048170	49.704971	64.459098
1661.913492	47.789602	64.464103
1661.127396	51.612485	64.469108
1660.849774	40.780647	64.474113
1660.484792	51.684835	64.479118
1659.942169	45.230062	64.484122
1659.332086	52.735491	64.489127
1658.664294	55.702234	64.494132
1658.753578	57.632516	64.499137
1657.103920	57.932539	64.504142
1656.746328	47.089747	64.509146
1656.096923	48.317374	64.514151
1655.169212	48.616249	64.519156
1654.354636	55.250587	64.524161
1653.532625	53.269782	64.529166
1652.969275	50.293846	64.534170
1652.720327	53.217707	64.539175
1652.179325	47.459679	64.544180
1651.971894	47.762401	64.549185
1650.941773	54.740058	64.554190
1650.123198	46.340621	64.559194
1649.686440	52.932285	64.564199
1648.137437	57.492947	64.569204
1647.257175	48.124038	64.574209
1646.747566	58.220168	64.579214
1646.943120	54.485017	64.584218
1646.754213	45.998167	64.589223
1645.678904	50.034152	64.594228
1645.004547	60.558572	64.599233
1643.793231	56.911304	64.604238
1643.464230	51.272560	64.609242
1642.833025	54.846918	64.614247
1642.217770	55.387891	64.619252
1641.250251	44.055385	64.624257
1640.182572	58.964641	64.629262
1639.717434	51.431559	64.634266
1639.435224	45.132537	64.639271
1638.652723	51.154664	64.644276
1638.541856	44.997153	64.649281
1637.731120	58.388011	64.654286
1636.742333	53.227816	64.659290
1636.034220	47.852726	64.664295
1635.263994	54.568330	64.669300
1635.015553	51.800986	64.674305
1634.082238	52.723645	64.679310
1633.325102	47.078804	64.684314
1632.652447	53.250638	64.689319
1631.926555	58.688199	64.694324
1631.582364	51.252597	64.699329
1630.736963	47.009475	64.704334
1630.482248	56.245109	64.709338
1629.683844	51.021557	64.714343
1628.320634	62.724573	64.719348
1628.304961	47.183420	64.724353
1627.402828	56.228601	64.729358
1627.132414	53.841634	64.734362
1626.637565	47.276779	64.739367
1625.378601	54.550993	64.744372
1624.936447	57.007243	64.749377
1624.441648	56.590812	64.754382
1623.777899	58.653343	64.759386
1622.801982	54.025687	64.764391
1621.946293	64.831230	64.769396
1621.816664	47.355947	64.774401
1620.995620	60.975525	64.779406
1620.451175	56.892744	64.784410
1619.471693	62.052059	64.789415
1618.802595	61.070396	64.794420
1618.439671	58.456857	64.799425
1618.062782	44.073791	64.804430
1617.215818	52.264976	64.809434
1616.315217	52.263096	64.814439
1615.379036	54.610180	64.819444
1615.137235	56.747599	64.824449
1614.510108	56.199232	64.829454
1613.337150	53.857889	64.834458
1612.659911	46.617130	64.839463
1611.925764	63.476102	64.844468
1611.694020	49.762243	64.849473
1610.588326	61.099506	64.854478
1610.615357	47.338229	64.859482
1610.513137	62.284915	64.864487
1609.100839	57.316594	64.869492
1608.720974	51.831014	64.874497
1608.071340	55.607000	64.879502
1607.071582	52.478064	64.884506
1606.087998	45.355364	64.889511
1605.297417	63.279842	64.894516
1605.186613	54.583469	64.899521
1604.769345	58.570116	64.904526
1604.208442	56.533651	64.909530
1603.044659	54.088355	64.914535
1602.016886	65.504705	64.919540
1601.766513	58.919932	64.924545
1601.484369	52.016941	64.929550
1600.745288	57.801951	64.934554
1600.221951	49.191625	64.939559
1599.187732	47.419594	64.944564
1598.838997	51.340159	64.949569
1597.360980	49.214446	64.954574
1596.519232	45.342911	64.959578
1596.252485	43.081521	64.964583
1595.715924	57.018593	64.969588
1595.530259	46.834464	64.974593
1594.935533	53.858078	64.979598
1594.468629	54.202030	64.984602
1593.217394	42.747472	64.989607
1592.336329	55.621240	64.994612
1592.309543	46.367485	64.999617
1590.960297	48.643013	65.004622
1590.346151	49.712092	65.009626
1589.680827	47.572376	65.014631
1589.049553	55.965838	65.019636
1588.876931	51.502298	65.024641
1588.308657	50.170317	65.029646
1587.339905	58.667863	65.034650
1586.656904	47.925676	65.039655
1585.809601	49.462301	65.044660
1585.780975	54.801701	65.049665
1584.515875	48.321393	65.054670
1583.481421	49.567639	65.059674
1583.491019	46.685188	65.064679
1582.918383	52.615639	65.069684
1582.317451	49.246731	65.074689
1581.159697	49.123298	65.079694
1580.518397	53.509812	65.084698
1580.303073	54.132332	65.089703
1579.804614	55.153071	65.094708
1578.934985	45.856620	65.099713
1577.774372	42.034180	65.104718
1577.390118	53.887588	65.109722
1577.221223	47.526418	65.114727
1575.786507	54.054307	65.119732
1575.004899	51.185609	65.124737
1574.506648	55.645588	65.129742
1574.112589	48.828193	65.134746
1573.963176	40.284622	65.139751
1572.747234	57.002527	65.144756
1572.424937	42.082533	65.149761
1571.225576	58.542344	65.154766
1571.020087	51.737564	65.159770
1569.853532	50.806572	65.164775
1568.664537	61.529467	65.169780
1568.229720	48.171157	65.174785
1567.836538	52.474095	65.179790
1567.560968	63.665281	65.184794
1567.410099	48.642350	65.189799
1566.682786	58.607501	65.194804
1565.757579	52.282926	65.199809
1564.773628	49.263459	65.204814
1564.449713	48.625927	65.209818
1563.355288	49.041209	65.214823
1562.358589	48.594155	65.219828
1562.068432	42.154487	65.224833
1561.434028	52.992681	65.229838
1561.131585	49.644158	65.234842
1560.722262	54.211432	65.239847
1559.603517	48.666652	65.244852
1558.810535	50.126846	65.249857
1558.404512	52.189440	65.254862
1557.722167	45.017320	65.259866
1556.530871	48.202883	65.264871
1555.846867	54.116342	65.269876
1555.381379	51.891266	65.274881
1554.980838	41.936830	65.279886
1554.412934	55.779537	65.284890
1553.858171	46.609681	65.289895
1552.838455	51.950445	65.294900
1552.514676	54.253857	65.299905
1551.547930	55.738511	65.304910
1551.099668	52.275967	65.309914
1550.426043	43.746309	65.314919
1549.257704	57.577196	65.319924
1548.825349	49.275698	65.324929
1548.420966	54.485573	65.329934
1548.094935	51.522416	65.334938
1547.139103	46.453218	65.339943
1546.137666	54.602736	65.344948
1545.877410	48.243471	65.349953
1545.323808	64.690570	65.354958
1544.414669	53.486020	65.359962
1543.488703	59.713894	65.364967
1542.812892	56.415240	65.369972
1542.466804	50.947960	65.374977
1541.931357	41.149004	65.379982
1541.086368	48.906237	65.384986
1540.343279	39.510854	65.389991
1539.598785	50.880619	65.394996
1539.089857	46.248180	65.400001
1538.872973	48.709644	65.405006
1537.538225	57.743169	65.410010
1537.156183	41.571140	65.415015
1536.363971	53.856798	65.420020
1536.082123	39.256813	65.425025
1534.876044	58.291240	65.430030
1534.482559	54.501456	65.435034
1534.331846	39.921633	65.440039
1533.628006	61.771486	65.445044
1532.538625	48.080393	65.450049
1531.461039	43.230820	65.455054
1530.933827	50.824021	65.460058
1530.824597	39.216417	65.465063
1529.886436	49.155150	65.470068
1528.903737	51.454463	65.475073
1528.241905	45.088054	65.480078
1527.790020	58.406137	65.485082
1527.725065	46.157569	65.490087
1526.641229	52.076223	65.495092
1525.684539	52.878057	65.500097
1525.377562	47.824029	65.505102
1524.732369	55.390251	65.510106
1524.268949	47.085813	65.515111
1522.808227	57.825093	65.520116
1522.300831	47.862412	65.525121
1522.153298	62.013633	65.530126
1521.498078	58.718020	65.535130
1520.668798	48.446950	65.540135
1519.532170	55.583498	65.545140
1519.436135	47.591256	65.550145
1519.046238	55.817064	65.555150
1518.155318	48.313831	65.560154
1517.326359	53.108640	65.565159
1516.420391	51.037147	65.570164
1516.335452	45.484222	65.575169
1515.112859	42.609930	65.580174
1514.125709	46.221954	65.585178
1513.841759	47.915077	65.590183
1512.975583	48.294109	65.595188
1513.026839	45.614771	65.600193
1512.537657	45.981201	65.605198
1511.636707	46.909798	65.610202
1510.966285	34.438921	65.615207
1510.249064	51.903891	65.620212
1509.179707	42.298598	65.625217
1508.338348	50.440032	65.630222
1507.635350	55.689481	65.635226
1507.630269	44.000672	65.640231
1507.082746	48.979412	65.645236
1506.442685	47.034397	65.650241
1505.337094	47.054094	65.655246
1504.721389	59.125635	65.660250
1504.299576	39.408706	65.665255
1503.208465	49.176214	65.670260
1502.489582	41.282960	65.675265
1501.956333	55.083893	65.680270
1501.079134	53.031487	65.685274
1501.466210	30.719717	65.690279
1500.072371	51.603749	65.695284
1499.384272	46.135640	65.700289
1498.865653	50.825942	65.705294
1498.256058	52.439934	65.710298
1497.900861	52.874958	65.715303
1496.635475	49.280514	65.720308
1496.473852	46.332238	65.725313
1495.341132	48.466173	65.730318
1494.958305	55.391474	65.735322
1494.406253	48.684359	65.740327
1493.213326	48.331594	65.745332
1492.975862	44.215834	65.750337
1492.623988	57.016561	65.755342
1491.413407	50.535524	65.760346
1490.641851	56.743604	65.765351
1489.807876	53.865909	65.770356
1489.414486	47.021621	65.775361
1489.383215	51.429474	65.780366
1488.501460	53.917759	65.785370
1487.936894	49.450289	65.790375
1487.049268	56.501546	65.795380
1486.526472	51.450284	65.800385
1485.310372	55.273744	65.805390
1484.543265	49.204771	65.810394
1484.103292	45.925426	65.815399
1483.788755	57.433451	65.820404
1483.309384	44.951136	65.825409
1482.297042	59.142022	65.830414
1481.727226	57.080195	65.835418
1481.283170	44.483461	65.840423
1480.183565	59.943446	65.845428
1479.681367	49.790719	65.850433
1478.594716	56.193955	65.855438
1477.959644	53.097000	65.860442
1477.751028	45.657234	65.865447
1477.117891	61.358472	65.870452
1476.534168	48.124779	65.875457
1475.366464	55.097550	65.880462
1475.055288	53.472428	65.885466
1475.126178	48.334701	65.890471
1473.858936	57.177755	65.895476
1472.908085	44.715183	65.900481
1472.535071	56.104770	65.905486
1472.194968	49.285131	65.910490
1470.800123	53.513889	65.915495
1469.945941	61.572222	65.920500
1469.641621	40.269171	65.925505
1468.965162	49.668020	65.930510
1468.460274	47.997994	65.935514
1468.311053	52.375708	65.940519
1467.089401	44.991293	65.945524
1466.470993	53.963035	65.950529
1465.993403	46.323173	65.955534
1465.138888	58.655018	65.960538
1464.449657	42.752603	65.965543
1463.721643	53.965225	65.970548
1463.560035	38.018382	65.975553
1462.223732	49.253563	65.980558
1461.434021	46.595922	65.985562
1461.041198	39.638015	65.990567
1460.525718	57.783701	65.995572
1460.042081	48.165762	66.000577
1459.285627	44.786914	66.005582
1458.495517	43.379837	66.010586
1458.185064	41.958026	66.015591
1457.434416	51.518478	66.020596
1456.784910	51.818938	66.025601
1456.167572	45.585827	66.030606
1455.102832	51.958779	66.035610
1454.779670	39.396459	66.040615
1453.584210	60.772527	66.045620
1452.866190	46.377497	66.050625
1452.271367	51.360610	66.055630
1451.846150	52.565269	66.060634
1451.981823	53.512052	66.065639
1450.630745	55.652326	66.070644
1449.887816	46.130795	66.075649
1449.545141	52.603447	66.080654
1448.823735	50.196723	66.085658
1447.881342	50.624159	66.090663
1446.898595	47.664473	66.095668
1446.467637	47.662123	66.100673
1446.136658	45.734230	66.105678
1445.465629	50.180687	66.110682
1444.608107	54.846018	66.115687
1443.560308	48.096290	66.120692
1443.428313	52.475997	66.125697
1443.137091	53.615206	66.130702
1442.053042	51.542084	66.135706
1441.399529	56.782106	66.140711
1440.698127	55.778818	66.145716
1440.392289	56.112967	66.150721
1439.552861	50.165890	66.155726
1438.592886	57.469929	66.160730
1438.372282	44.085501	66.165735
1437.386194	58.079838	66.170740
1436.669343	45.766169	66.175745
1435.485156	57.120688	66.180750
1435.139519	52.000280	66.185754
1434.699897	40.360052	66.190759
1434.538003	47.860506	66.195764
1433.449063	45.854396	66.200769
1432.672962	44.541293	66.205774
1431.998531	52.378676	66.210778
1432.088393	40.181213	66.215783
1430.699779	52.951182	66.220788
1429.938760	43.079306	66.225793
1429.235730	45.871931	66.230798
1428.551784	53.879558	66.235802
1428.579770	42.358967	66.240807
1428.107526	54.740440	66.245812
1426.976177	49.435844	66.250817
1426.716709	47.189088	66.255822
1425.337228	51.784425	66.260826
1424.505279	47.673281	66.265831
1424.111263	55.712095	66.270836
1423.735488	46.662062	66.275841
1423.132113	39.351284	66.280846
1422.167114	53.818500	66.285850
1421.440326	39.308192	66.290855
1420.700935	55.067316	66.295860
1420.760553	38.429320	66.300865
1419.551290	43.931138	66.305870
1418.588678	49.855793	66.310874
1418.445673	41.792187	66.315879
1417.718208	50.672461	66.320884
1417.003902	53.271344	66.325889
1416.273075	52.367357	66.330894
1415.310742	52.939897	66.335898
1415.002504	42.724826	66.340903
1414.866760	46.622590	66.345908
1413.627394	50.661085	66.350913
1412.750356	41.764849	66.355918
1412.488642	54.749935	66.360922
1412.019965	43.816059	66.365927
1410.606692	45.859008	66.370932
1409.952453	40.013395	66.375937
1409.617019	43.105555	66.380942
1409.292161	53.129757	66.385946
1408.690009	42.201331	66.390951
1407.376930	53.786075	66.395956
1407.055465	40.685766	66.400961
1406.542246	45.775760	66.405966
1405.847018	44.990694	66.410970
1405.122307	44.215046	66.415975
1404.159099	38.785970	66.420980
1403.835330	47.799190	66.425985
1403.104738	47.264169	66.430990
1402.113112	47.693140	66.435994
1401.718229	50.936674	66.440999
1401.014740	45.333852	66.446004
1400.692526	36.492932	66.451009
1399.848937	44.659973	66.456014
1398.869921	41.526254	66.461018
1398.614519	36.921361	66.466023
1398.078742	48.943931	66.471028
1397.416830	43.648308	66.476033
1396.695007	41.044552	66.481038
1396.046164	41.392230	66.486042
1395.037971	45.286754	66.491047
1394.224585	46.203048	66.496052
1393.414472	37.824453	66.501057
1393.376480	42.520368	66.506062
1392.851886	56.859240	66.511066
1391.864869	47.313454	66.516071
1390.954217	47.376328	66.521076
1390.665911	47.986810	66.526081
1390.343652	43.592812	66.531086
1389.070733	44.214733	66.536090
1388.463573	37.286185	66.541095
1387.741999	52.364402	66.546100
1387.465475	38.235112	66.551105
1386.728031	47.593206	66.556110
1385.820708	45.764824	66.561114
1385.280136	37.832231	66.566119
1384.547947	48.550372	66.571124
1383.737109	48.179497	66.576129
1382.952775	46.117104	66.581134
1382.388113	49.270937	66.586138
1382.173772	47.007552	66.591143
1381.510242	37.456085	66.596148
1380.483218	47.093597	66.601153
1379.955501	45.766257	66.606158
1379.317634	50.689995	66.611162
1379.124183	37.250809	66.616167
1378.199044	51.328503	66.621172
1377.308075	49.615793	66.626177
1376.975749	31.991465	66.631182
1375.616110	49.448182	66.636186
1374.976046	37.883991	66.641191
1374.155107	48.561050	66.646196
1373.881670	39.100535	66.651201
1373.613465	42.800164	66.656206
1372.877922	46.908392	66.661210
1372.234882	48.554535	66.666215
1371.221427	42.698229	66.671220
1370.467951	48.565998	66.676225
1370.564069	44.201687	66.681230
1369.413282	47.975390	66.686234
1368.623033	45.693173	66.691239
1368.096270	37.408314	66.696244
1367.770989	46.976850	66.701249
1366.803238	35.802217	66.706254
1365.623473	48.797623	66.711258
1365.208279	41.419102	66.716263
1364.792324	41.397035	66.721268
1364.489088	52.926913	66.726273
1364.064672	45.882586	66.731278
1363.244778	48.252268	66.736282
1362.217664	42.724560	66.741287
1361.015247	46.686242	66.746292
1360.429138	49.602220	66.751297
1360.034830	51.533671	66.756302
1359.461052	43.213708	66.761306
1359.356647	52.422290	66.766311
1358.340015	54.003251	66.771316
1357.728560	42.005593	66.776321
1356.627871	37.629699	66.781326
1355.493137	47.022573	66.786330
1355.178679	38.995696	66.791335
1354.662607	48.698642	66.796340
1354.034451	46.526276	66.801345
1353.828788	42.343980	66.806350
1353.179616	55.896851	66.811354
1352.854104	31.760342	66.816359
1352.113251	47.800390	66.821364
1351.008585	45.796817	66.826369
1350.036273	47.293466	66.831374
1349.250762	46.682037	66.836378
1349.478386	45.825968	66.841383
1348.183564	42.375053	66.846388
1347.167459	47.000966	66.851393
1346.908261	42.093914	66.856398
1346.402214	52.156383	66.861402
1345.858930	40.507431	66.866407
1344.704724	41.088423	66.871412
1344.169910	37.079881	66.876417
1344.002547	37.519756	66.881422
1342.982492	47.558286	66.886426
1342.347073	36.628868	66.891431
1341.550492	47.275253	66.896436
1341.379043	40.889293	66.901441
1340.468295	38.500090	66.906446
1339.369639	54.196493	66.911450
1339.256963	38.133093	66.916455
1338.139968	32.023615	66.921460
1337.934575	48.550958	66.926465
1336.750195	48.446061	66.931470
1336.065752	40.531623	66.936474
1335.847594	41.679727	66.941479
1335.186060	41.225208	66.946484
1334.511239	44.786061	66.951489
1333.669399	37.888532	66.956494
1332.780504	40.909421	66.961498
1332.653825	36.771341	66.966503
1331.842125	48.088745	66.971508
1331.162301	35.693549	66.976513
1330.590363	48.950292	66.981518
1329.621913	46.051459	66.986522
1329.387911	42.080248	66.991527
1328.219214	41.264825	66.996532
1327.473774	44.611408	67.001537
1327.475327	45.218391	67.006542
1326.426703	49.745405	67.011546
1325.480633	37.782038	67.016551
1324.658380	57.711107	67.021556
1324.385120	43.174465	67.026561
1323.987731	51.168089	67.031566
1323.409284	50.151595	67.036570
1323.180607	41.228010	67.041575
1321.861876	47.097351	67.046580
1321.421046	62.022143	67.051585
1320.453337	49.418825	67.056590
1319.348186	58.453785	67.061594
1319.281464	48.430565	67.066599
1318.674569	58.307229	67.071604
1318.367657	42.697325	67.076609
1317.406802	58.179444	67.081614
1316.315285	53.414184	67.086618
1316.070098	45.344760	67.091623
1314.738557	53.985213	67.096628
1314.193999	57.478056	67.101633
1313.770591	47.282894	67.106638
1312.975936	44.099398	67.111642
1312.929113	44.228381	67.116647
1312.891697	51.802082	67.121652
1311.741904	47.353591	67.126657
1310.962437	41.635150	67.131662
1309.764154	66.045699	67.136666
1309.366569	44.022682	67.141671
1308.820607	39.754152	67.146676
1307.918015	47.651483	67.151681
1306.834067	48.270207	67.156686
1305.836617	41.827927	67.161690
1305.712107	48.081400	67.166695
1305.063556	54.831348	67.171700
1304.801616	51.099541	67.176705
1304.854735	43.627652	67.181710
1303.435948	58.778891	67.186714
1303.076822	53.523462	67.191719
1302.271622	45.953078	67.196724
1300.903542	46.306327	67.201729
1300.439904	45.676853	67.206734
1299.940988	50.767744	67.211738
1299.535210	49.261764	67.216743
1299.248344	46.118960	67.221748
1298.160031	45.394846	67.226753
1297.796753	53.271088	67.231758
1296.569106	60.972536	67.236762
1295.696576	49.476865	67.241767
1295.198950	48.920604	67.246772
1294.594624	45.765198	67.251777
1294.214493	53.155275	67.256782
1293.741598	49.228358	67.261786
1293.323407	46.721433	67.266791
1291.800291	62.059576	67.271796
1291.265911	60.804275	67.276801
1291.200828	53.898367	67.281806
1290.002030	50.211445	67.286810
1289.891707	43.669119	67.291815
1288.642047	57.557168	67.296820
1288.343301	46.414963	67.301825
1287.223331	54.736366	67.306830
1286.820998	47.447277	67.311834
1286.584084	51.097784	67.316839
1285.642816	51.491985	67.321844
1284.526415	44.521436	67.326849
1284.132100	41.211220	67.331854
1283.606754	55.446138	67.336858
1283.079496	43.447734	67.341863
1281.922950	52.087183	67.346868
1281.500081	50.525578	67.351873
1281.168356	46.607757	67.356878
1280.444541	48.563226	67.361882
1279.315872	49.088149	67.366887
1278.620959	51.272407	67.371892
1278.371418	52.384506	67.376897
1278.012800	45.219354	67.381902
1276.696071	41.267348	67.386906
1276.376510	48.688793	67.391911
1275.637918	43.320248	67.396916
1275.159935	38.523688	67.401921
1274.059513	39.080391	67.406926
1272.995816	49.083305	67.411930
1273.103168	48.052391	67.416935
1272.506504	60.705967	67.421940
1271.987548	42.392261	67.426945
1270.982092	50.943035	67.431950
1270.158343	51.931977	67.436954
1269.768974	48.007553	67.441959
1269.305917	39.219018	67.446964
1268.319670	44.105132	67.451969
1267.884324	42.299515	67.456974
1266.892742	48.466937	67.461978
1266.670718	48.820894	67.466983
1265.633263	39.601733	67.471988
1265.085922	51.939960	67.476993
1264.951974	50.236225	67.481998
1263.376772	60.060291	67.487002
1263.247232	47.342651	67.492007
1262.380483	46.001439	67.497012
1261.743089	42.349842	67.502017
1261.038900	38.891789	67.507022
1259.866693	57.905130	67.512026
1259.417295	46.444696	67.517031
1259.087495	53.325312	67.522036
1258.993922	44.990522	67.527041
1258.070347	47.368837	67.532046
1257.199695	63.145706	67.537050
1256.718820	42.376993	67.542055
1255.971584	58.941615	67.547060
1254.881407	56.601473	67.552065
1254.543557	48.430102	67.557070
1253.576858	58.559526	67.562074
1253.406361	46.562746	67.567079
1252.311265	50.467987	67.572084
1251.688794	42.247263	67.577089
1251.556048	42.460871	67.582094
1250.762879	46.245562	67.587098
1250.054696	42.728224	67.592103
1249.132367	59.420036	67.597108
1248.623387	50.914762	67.602113
1247.509063	52.407223	67.607118
1246.556031	53.676922	67.612122
1246.467283	49.819814	67.617127
1245.617754	51.052555	67.622132
1245.619550	52.529957	67.627137
1245.016811	45.441478	67.632142
1243.690325	50.555167	67.637146
1243.546106	43.378008	67.642151
1242.613464	49.115028	67.647156
1241.804748	49.270552	67.652161
1241.360740	43.364753	67.657166
1240.650205	55.257437	67.662170
1240.027548	48.638894	67.667175
1239.155991	47.989145	67.672180
1238.478758	45.998075	67.677185
1237.819384	49.794610	67.682190
1237.307433	41.516894	67.687194
1237.078817	38.300184	67.692199
1235.855807	49.086939	67.697204
1235.140954	45.878165	67.702209
1234.959728	45.216409	67.707214
1233.540039	46.705397	67.712218
1232.903083	50.030023	67.717223
1232.474489	44.978041	67.722228
1231.881621	51.523608	67.727233
1231.920449	46.458796	67.732238
1231.197424	48.846227	67.737242
1230.488373	53.612584	67.742247
1229.608551	48.846819	67.747252
1228.996499	41.726712	67.752257
1227.822826	47.880526	67.757262
1227.189912	46.358642	67.762266
1226.787114	39.422875	67.767271
1226.546929	37.654039	67.772276
1225.219513	43.825994	67.777281
1224.644655	41.716149	67.782286
1223.943460	45.162953	67.787290
1223.693380	42.903692	67.792295
1222.625473	46.240082	67.797300
1221.854844	45.864442	67.802305
1221.795224	45.604386	67.807310
1220.852925	48.230113	67.812314
1219.920365	46.021038	67.817319
1219.227209	50.333871	67.822324
1218.626436	47.258343	67.827329
1218.207530	38.748223	67.832334
1217.745283	51.299997	67.837338
1216.955286	41.901162	67.842343
1216.260645	55.300432	67.847348
1215.690586	53.412170	67.852353
1215.569355	41.806527	67.857358
1214.416641	47.353054	67.862362
1213.626394	47.653880	67.867367
1212.391780	49.077178	67.872372
1211.889957	47.282143	67.877377
1211.542014	48.988625	67.882382
1210.525548	50.725730	67.887386
1210.449023	42.014508	67.892391
1209.495515	52.447763	67.897396
1208.670781	38.139205	67.902401
1208.275399	51.645419	67.907406
1207.655349	45.017011	67.912410
1207.446547	45.307370	67.917415
1206.541163	50.999067	67.922420
1205.775932	40.102957	67.927425
1204.818614	42.729501	67.932430
1203.631009	59.152855	67.937434
1203.273226	44.826800	67.942439
1202.945584	46.780784	67.947444
1202.561987	36.880521	67.952449
1202.456261	38.349790	67.957454
1201.022137	42.395696	67.962458
1200.577501	41.359528	67.967463
1199.575000	40.024159	67.972468
1198.467054	43.603464	67.977473
1197.708231	33.597301	67.982478
1197.094859	39.223633	67.987482
1196.867437	34.300515	67.992487
1196.555918	39.722727	67.997492
1196.137601	32.281673	68.002497
1195.265663	30.771004	68.007502
1194.111134	44.279675	68.012506
1193.841341	29.851338	68.017511
1193.493646	48.594787	68.022516
1192.456581	43.959698	68.027521
1191.887455	36.471666	68.032526
1190.876693	52.704469	68.037530
1190.439848	40.532451	68.042535
1189.415632	52.389875	68.047540
1188.997350	44.310158	68.052545
1188.884482	46.704638	68.057550
1188.208336	44.683450	68.062554
1187.191448	46.701322	68.067559
1186.509767	43.167174	68.072564
1185.904520	45.848115	68.077569
1184.717624	46.577877	68.082574
1183.902100	44.556780	68.087578
1183.756817	33.514780	68.092583
1183.107387	44.937287	68.097588
1182.851298	44.464056	68.102593
1182.365454	40.299535	68.107598
1181.293008	36.135272	68.112602
1180.828652	43.396824	68.117607
1179.729821	45.161233	68.122612
1178.963612	35.976248	68.127617
1178.720180	41.729824	68.132622
1178.255841	37.211809	68.137626
1177.255132	42.697904	68.142631
1176.466221	40.059157	68.147636
1175.693910	50.056757	68.152641
1175.589401	37.325700	68.157646
1174.433165	51.810766	68.162650
1173.754933	38.193268	68.167655
1173.219806	43.720431	68.172660
1172.788958	37.413598	68.177665
1171.873211	44.907789	68.182670
1170.792359	49.266525	68.187674
1170.841609	38.917388	68.192679
1170.320510	39.927609	68.197684
1169.323098	44.222611	68.202689
1168.469154	38.000418	68.207694
1167.980278	44.701336	68.212698
1167.229968	41.871952	68.217703
1166.249582	48.272586	68.222708
1165.309382	39.003317	68.227713
1165.011461	49.321273	68.232718
1164.450832	53.904771	68.237722
1164.225634	43.217668	68.242727
1163.941271	39.807988	68.247732
1163.053210	50.651882	68.252737
1162.432896	47.830207	68.257742
1161.189325	51.136216	68.262746
1160.600256	40.620528	68.267751
1160.008712	41.910031	68.272756
1159.788959	40.943757	68.277761
1159.185085	41.722724	68.282766
1157.824182	43.882053	68.287770
1157.691315	48.131015	68.292775
1156.903870	38.487378	68.297780
1155.021417	44.459069	68.302785
1154.960969	37.446792	68.307790
1154.184190	42.629202	68.312794
1154.298425	40.939617	68.317799
1154.023717	39.034358	68.322804
1153.254313	47.911888	68.327809
1152.476863	35.548062	68.332814
1151.515964	42.923286	68.337818
1150.688929	34.492292	68.342823
1149.736135	30.225438	68.347828
1149.365694	39.012700	68.352833
1149.320394	29.487568	68.357838
1148.362659	46.964011	68.362842
1147.161070	43.820067	68.367847
1146.761969	41.551403	68.372852
1146.258126	52.469805	68.377857
1145.768560	34.328100	68.382862
1144.489623	45.005513	68.387866
1144.029178	49.005387	68.392871
1143.654962	40.625369	68.397876
1143.065198	47.377030	68.402881
1142.241856	38.382491	68.407886
1141.008221	44.865989	68.412890
1140.689629	45.716276	68.417895
1140.478096	40.390100	68.422900
1139.507573	55.044332	68.427905
1138.759585	32.214563	68.432910
1137.940318	51.758401	68.437914
1137.933671	40.021009	68.442919
1137.701405	38.872228	68.447924
1136.661472	40.461710	68.452929
1136.060251	46.663274	68.457934
1134.733511	40.126798	68.462938
1134.119152	44.576921	68.467943
1133.259605	44.702718	68.472948
1132.740396	46.162068	68.477953
1132.657425	47.288683	68.482958
1131.440577	53.851519	68.487962
1131.006382	50.339520	68.492967
1130.207253	43.774314	68.497972
1129.888926	52.928602	68.502977
1129.348158	38.160184	68.507982
1128.035114	49.978410	68.512986
1127.701692	44.244279	68.517991
1127.092193	40.140440	68.522996
1126.147931	36.815232	68.528001
1125.747086	49.664740	68.533006
1125.074140	53.789881	68.538010
1124.933221	34.998229	68.543015
1123.766834	44.454560	68.548020
1122.656743	42.921875	68.553025
1122.791376	43.717418	68.558030
1121.582375	52.144500	68.563034
1120.758987	37.843654	68.568039
1120.204297	46.701229	68.573044
1119.799213	47.426508	68.578049
1119.615609	44.409227	68.583054
1118.340534	50.840983	68.588058
1117.674555	35.179455	68.593063
1117.359155	43.656775	68.598068
1116.573289	41.880136	68.603073
1115.592232	37.460098	68.608078
1114.804507	49.040230	68.613082
1114.626540	44.301637	68.618087
1114.182717	47.411068	68.623092
1113.022261	41.828995	68.628097
1112.388021	40.643236	68.633102
1111.640904	43.961756	68.638106
1111.553975	42.438207	68.643111
1110.454605	46.478219	68.648116
1109.783989	45.329784	68.653121
1109.065493	42.446475	68.658126
1108.650802	48.492220	68.663130
1108.057914	41.634025	68.668135
1107.237427	46.585287	68.673140
1106.535601	41.988373	68.678145
1106.232832	32.603547	68.683150
1104.573319	51.585628	68.688154
1104.370315	36.519071	68.693159
1103.678529	39.016679	68.698164
1103.148815	44.181878	68.703169
1102.982596	37.762006	68.708174
1102.095266	49.946174	68.713178
1101.620115	36.826246	68.718183
1101.102323	45.605416	68.723188
1099.517949	39.969362	68.728193
1099.055881	31.800449	68.733198
1098.279852	43.132720	68.738202
1098.095927	31.360465	68.743207
1097.429097	41.281372	68.748212
1096.418931	39.702843	68.753217
1096.243683	30.263042	68.758222
1095.347930	43.514540	68.763226
1094.733685	39.392543	68.768231
1094.253207	41.192659	68.773236
1093.425390	39.424279	68.778241
1093.039670	43.115811	68.783246
1091.584830	41.283177	68.788250
1091.288483	38.931947	68.793255
1090.562752	49.634919	68.798260
1090.274926	41.184401	68.803265
1089.427238	39.231530	68.808270
1088.251650	39.565309	68.813274
1088.106974	35.811730	68.818279
1087.722387	36.571598	68.823284
1086.644507	34.954961	68.828289
1086.060024	37.788732	68.833294
1085.501496	44.007166	68.838298
1084.798542	38.194639	68.843303
1083.968651	38.418234	68.848308
1083.048962	46.589574	68.853313
1082.960550	40.532632	68.858318
1082.340496	53.342901	68.863322
1081.930022	38.883348	68.868327
1080.799692	44.393250	68.873332
1080.250186	41.306452	68.878337
1079.776124	38.412652	68.883342
1078.423737	42.477157	68.888346
1077.852537	48.755956	68.893351
1077.388371	37.689009	68.898356
1077.004840	43.083262	68.903361
1076.198259	47.051480	68.908366
1074.968713	42.048107	68.913370
1074.933463	38.999347	68.918375
1074.798391	35.570662	68.923380
1073.746123	44.193592	68.928385
1072.952678	35.094983	68.933390
1072.323626	36.231203	68.938394
1071.664110	39.590989	68.943399
1070.412520	38.962334	68.948404
1069.720602	41.300704	68.953409
1069.597428	28.515875	68.958414
1068.807377	45.874193	68.963418
1068.777982	33.957513	68.968423
1067.672458	41.034078	68.973428
1066.838095	43.240572	68.978433
1066.520076	34.200370	68.983438
1064.777297	39.588518	68.988442
1064.338202	43.204969	68.993447
1064.057367	37.863023	68.998452
1063.552522	39.614982	69.003457
1063.433003	35.534136	69.008462
1062.495140	36.795179	69.013466
1061.755238	36.400507	69.018471
1061.251892	30.324429	69.023476
1060.268736	45.777020	69.028481
1059.596213	41.085577	69.033486
1058.663901	44.495073	69.038490
1058.183661	32.511351	69.043495
1057.887156	41.649547	69.048500
1057.055822	42.450531	69.053505
1056.778143	34.204986	69.058510
1055.665845	46.740335	69.063514
1055.199525	49.572663	69.068519
1054.037333	37.479817	69.073524
1053.232103	40.224139	69.078529
1052.831777	34.658361	69.083534
1052.770709	42.273648	69.088538
1052.371032	40.058708	69.093543
1051.241057	48.492165	69.098548
1050.710835	43.595162	69.103553
1049.532290	43.962545	69.108558
1049.118653	40.018374	69.113562
1048.845794	41.821736	69.118567
1048.419822	34.913355	69.123572
1046.848846	43.934199	69.128577
1046.315901	35.145809	69.133582
1045.560230	53.206704	69.138586
1045.185896	47.275674	69.143591
1044.065572	39.938454	69.148596
1043.410412	36.903168	69.153601
1043.275247	34.281881	69.158606
1042.837340	41.771045	69.163610
1042.142665	42.310601	69.168615
1041.288975	43.099379	69.173620
1040.510716	52.733686	69.178625
1039.963733	42.357996	69.183630
1038.642276	45.320068	69.188634
1038.384614	38.977829	69.193639
1038.094956	39.661102	69.198644
1037.035797	47.395762	69.203649
1036.297676	32.756553	69.208654
1035.600732	37.402754	69.213658
1034.859957	45.356412	69.218663
1034.791590	33.108478	69.223668
1034.175837	32.921138	69.228673
1033.270516	34.676895	69.233678
1032.619069	39.705357	69.238682
1032.355760	41.317971	69.243687
1031.362574	37.015015	69.248692
1030.655054	37.925616	69.253697
1029.880584	36.342730	69.258702
1029.200968	31.488429	69.263706
1028.200448	29.052131	69.268711
1027.765827	41.533279	69.273716
1026.799198	37.256060	69.278721
1026.727932	31.262630	69.283726
1026.267792	36.016233	69.288730
1025.424400	26.920865	69.293735
1024.552409	31.467187	69.298740
1024.267379	38.175110	69.303745
1023.955658	30.262988	69.308750
1022.637176	40.088895	69.313754
1021.494217	30.828305	69.318759
1021.570911	35.124344	69.323764
1020.839967	41.907946	69.328769
1019.989658	30.970266	69.333774
1019.502299	44.211995	69.338778
1018.825838	35.274564	69.343783
1017.714917	42.476583	69.348788
1017.008641	44.703713	69.353793
1016.817582	31.541771	69.358798
1015.827106	40.624806	69.363802
1015.448292	32.945704	69.368807
1015.087042	35.772356	69.373812
1014.260291	37.447812	69.378817
1013.825263	35.765193	69.383822
1012.459521	38.781630	69.388826
1011.704659	36.719403	69.393831
1011.224071	39.126662	69.398836
1010.671472	36.822524	69.403841
1010.486837	33.117887	69.408846
1009.898643	43.303834	69.413850
1009.399642	38.359299	69.418855
1008.117034	42.911040	69.423860
1007.067616	39.947956	69.428865
1006.473677	37.828588	69.433870
1005.871987	43.746403	69.438874
1005.670980	36.403277	69.443879
1005.137922	39.165807	69.448884
1003.964007	44.867172	69.453889
1003.931254	38.684691	69.458894
1002.837191	43.414587	69.463898
1001.871839	41.182432	69.468903
1001.220905	30.195693	69.473908
1000.846474	46.865010	69.478913
1000.648893	29.394406	69.483918
999.646353	43.325218	69.488922
998.633867	40.791489	69.493927
998.298714	43.732261	69.498932
997.453594	46.795175	69.503937
997.220383	48.060814	69.508942
995.982494	47.500977	69.513946
995.396764	39.820108	69.518951
995.106921	46.489378	69.523956
994.123540	39.493086	69.528961
993.271910	33.286367	69.533966
992.805718	43.049213	69.538970
992.170790	40.658833	69.543975
992.077556	35.816892	69.548980
991.419076	34.480485	69.553985
990.391065	42.572892	69.558990
990.032587	46.867214	69.563994
988.990728	40.085228	69.568999
988.237145	37.519769	69.574004
987.555904	44.721237	69.579009
987.091832	35.839907	69.584014
985.905283	47.311637	69.589018
985.050389	40.561403	69.594023
984.956917	28.046246	69.599028
984.251539	40.300825	69.604033
984.344816	41.085594	69.609038
983.001292	42.426983	69.614042
982.427313	34.963442	69.619047
981.947304	36.030238	69.624052
980.898997	42.823348	69.629057
980.098863	34.787105	69.634062
979.085001	46.928355	69.639066
978.963070	29.300643	69.644071
979.005128	32.231853	69.649076
978.098304	40.528901	69.654081
977.310878	29.962849	69.659086
976.459610	45.011281	69.664090
976.106204	37.965216	69.669095
974.903734	44.018057	69.674100
974.100242	46.071438	69.679105
973.870001	42.279445	69.684110
973.320889	39.869108	69.689114
972.654259	42.361169	69.694119
971.898956	34.499141	69.699124
971.381452	51.618572	69.704129
970.654375	30.066026	69.709134
969.491915	45.450976	69.714138
968.832348	32.322596	69.719143
968.369695	41.796306	69.724148
967.865009	44.461290	69.729153
966.985572	34.873374	69.734158
966.660106	53.554930	69.739162
966.372364	42.289633	69.744167
965.502038	35.609671	69.749172
964.088013	55.003752	69.754177
963.983421	36.480744	69.759182
963.506110	45.926828	69.764186
962.696455	46.289165	69.769191
961.769819	35.297424	69.774196
961.114050	48.009308	69.779201
960.961993	36.478004	69.784206
960.130224	46.871448	69.789210
959.214747	36.313160	69.794215
958.618701	40.795094	69.799220
957.910528	43.266963	69.804225
956.709199	45.979730	69.809230
955.980292	45.253765	69.814234
955.856288	48.115211	69.819239
955.313812	37.615836	69.824244
954.785807	56.517278	69.829249
954.383759	41.017238	69.834254
953.400873	47.940294	69.839258
952.908133	37.535505	69.844263
952.021760	49.117173	69.849268
950.990742	47.993019	69.854273
950.695597	36.866099	69.859278
950.272740	43.020387	69.864282
949.434771	42.501009	69.869287
948.457987	42.088875	69.874292
947.733318	47.375007	69.879297
947.612961	38.538335	69.884302
947.126305	30.696644	69.889306
945.958951	45.140963	69.894311
945.470859	37.010923	69.899316
944.830995	42.434942	69.904321
944.256280	38.805002	69.909326
943.033520	46.348114	69.914330
942.572266	32.811303	69.919335
942.217724	40.605745	69.924340
941.283236	38.632048	69.929345
940.748722	42.126508	69.934350
940.260288	48.144582	69.939354
939.764585	31.792158	69.944359
939.015042	43.303165	69.949364
937.767438	45.898728	69.954369
937.479318	42.103336	69.959374
936.815942	46.730028	69.964378
935.839526	47.133104	69.969383
934.959650	47.801508	69.974388
934.474680	39.945355	69.979393
934.274769	44.708021	69.984398
933.502297	48.965733	69.989402
933.377727	50.860622	69.994407
932.593324	40.436022	69.999412
931.385569	45.803766	70.004417
930.986285	47.244068	70.009422
929.742166	48.380437	70.014426
929.133999	38.656328	70.019431
928.884007	42.649545	70.024436
928.509418	46.251019	70.029441
928.147204	34.194941	70.034446
926.978415	39.313639	70.039450
926.623477	42.822100	70.044455
925.582385	47.362253	70.049460
924.842654	44.125998	70.054465
924.044788	42.428602	70.059470
923.520444	46.689404	70.064474
923.154841	45.352135	70.069479
922.337550	31.684341	70.074484
921.682011	36.294017	70.079489
921.042058	42.640547	70.084494
919.839760	42.368390	70.089498
919.190767	29.041237	70.094503
918.910063	40.032942	70.099508
918.464385	35.168252	70.104513
918.094702	36.324732	70.109518
917.232001	44.524892	70.114522
916.187979	42.485060	70.119527
915.885105	32.059532	70.124532
914.724512	49.645573	70.129537
913.986586	41.910104	70.134542
913.422681	44.354293	70.139546
912.756293	43.213126	70.144551
912.691489	45.451731	70.149556
911.785464	40.840073	70.154561
910.995748	42.984317	70.159566
910.458680	47.436376	70.164570
910.016269	45.699759	70.169575
908.931439	48.089663	70.174580
908.100202	45.792048	70.179585
908.047383	40.382301	70.184590
907.559314	46.023437	70.189594
906.433655	31.184198	70.194599
905.913984	38.356811	70.199604
904.866006	39.353168	70.204609
904.617606	44.092014	70.209614
903.287013	48.049061	70.214618
902.731656	48.735212	70.219623
902.961322	40.579257	70.224628
901.852790	46.205604	70.229633
901.251110	42.914272	70.234638
900.421641	58.407105	70.239642
900.143091	51.357021	70.244647
899.320788	45.495742	70.249652
898.037850	49.640744	70.254657
898.027954	45.337465	70.259662
897.233625	45.938651	70.264666
896.625746	40.327093	70.269671
895.631152	31.008269	70.274676
895.123559	39.103030	70.279681
894.891625	44.261868	70.284686
893.797441	53.590104	70.289690
892.874699	42.359658	70.294695
892.712399	43.998785	70.299700
892.000539	54.429934	70.304705
891.423273	43.262772	70.309710
890.314737	41.621139	70.314714
890.017276	48.424088	70.319719
889.578585	39.915625	70.324724
888.196449	51.115754	70.329729
887.580972	45.335099	70.334734
887.174894	34.397736	70.339738
886.950248	50.783024	70.344743
886.279798	38.689282	70.349748
885.163912	45.157299	70.354753
884.950241	43.683895	70.359758
884.159814	37.251440	70.364762
883.325486	42.958728	70.369767
882.898750	29.966788	70.374772
882.086174	41.044723	70.379777
881.298274	28.337344	70.384782
880.417366	50.261113	70.389786
879.647862	33.799328	70.394791
879.443956	41.643913	70.399796
878.914523	41.515411	70.404801
878.223052	34.139986	70.409806
877.338071	43.108504	70.414810
876.848063	49.998869	70.419815
875.915250	43.699461	70.424820
874.928190	39.263137	70.429825
874.668457	50.749816	70.434830
874.238005	46.521359	70.439834
873.731281	40.442711	70.444839
872.798334	49.827288	70.449844
871.952531	50.160716	70.454849
871.596437	36.481035	70.459854
870.243144	47.511002	70.464858
869.699357	45.085650	70.469863
869.190399	42.416640	70.474868
868.585658	45.838716	70.479873
868.393153	37.051385	70.484878
867.739194	50.166683	70.489882
866.748957	43.220424	70.494887
866.217427	43.253103	70.499892
865.502773	48.857773	70.504897
865.184347	36.835740	70.509902
864.089192	47.376781	70.514906
863.715498	43.713289	70.519911
863.049599	36.023147	70.524916
861.725166	47.327638	70.529921
861.485353	36.702852	70.534926
861.113207	55.420217	70.539930
859.838269	44.901839	70.544935
859.254382	35.325275	70.549940
858.656959	44.408872	70.554945
858.440147	36.018064	70.559950
857.764252	41.659141	70.564954
856.836234	41.269242	70.569959
856.166604	35.576066	70.574964
855.522079	51.786917	70.579969
855.441875	36.617299	70.584974
854.235492	42.796965	70.589978
853.453800	46.264554	70.594983
853.059000	40.639593	70.599988
852.266437	48.850685	70.604993
851.312578	43.183826	70.609998
850.732398	47.201222	70.615002
850.475351	34.915542	70.620007
849.725062	40.265694	70.625012
848.254656	46.801195	70.630017
848.135210	43.521425	70.635022
847.727614	46.186745	70.640026
846.999336	42.306892	70.645031
846.976729	41.206768	70.650036
845.656448	42.749528	70.655041
845.098617	40.744298	70.660046
844.475749	38.430886	70.665050
843.378879	48.732517	70.670055
842.888585	30.293017	70.675060
842.354531	44.177681	70.680065
842.250366	41.849511	70.685070
841.051111	42.966166	70.690074
840.245013	49.548890	70.695079
840.180039	37.267329	70.700084
838.710541	46.909203	70.705089
838.071524	46.865960	70.710094
837.735954	42.385872	70.715098
837.278568	47.635791	70.720103
837.099043	34.079401	70.725108
835.693618	45.540291	70.730113
835.342541	33.673273	70.735118
833.977215	46.184311	70.740122
833.169966	37.274074	70.745127
832.871529	46.978694	70.750132
832.390342	46.924521	70.755137
832.194395	40.963567	70.760142
831.520392	38.992603	70.765146
830.682926	43.765296	70.770151
829.892525	35.304953	70.775156
829.245789	45.165936	70.780161
827.995379	34.389800	70.785166
827.372790	31.153857	70.790170
826.978782	44.831731	70.795175
826.729489	46.812706	70.800180
826.178918	54.313523	70.805185
825.119564	39.503193	70.810190
824.556958	38.066417	70.815194
824.017476	48.545825	70.820199
823.308309	41.848151	70.825204
821.996787	47.148884	70.830209
821.590510	43.610431	70.835214
821.221256	39.574090	70.840218
820.966132	39.288397	70.845223
820.302051	33.488698	70.850228
819.249486	50.467805	70.855233
818.759988	43.310975	70.860238
817.538913	45.065032	70.865242
816.748552	49.016547	70.870247
816.493899	36.910261	70.875252
816.010991	50.670099	70.880257
815.484933	44.567735	70.885262
814.577230	44.721806	70.890266
813.894437	35.202002	70.895271
813.668557	42.513936	70.900276
812.493086	40.715842	70.905281
812.109025	40.622558	70.910286
811.225099	45.552460	70.915290
811.075053	39.273552	70.920295
810.091494	44.457428	70.925300
808.788225	46.095267	70.930305
808.443868	38.979990	70.935310
808.252741	43.063190	70.940314
807.526578	44.948196	70.945319
806.710187	35.307740	70.950324
805.752547	34.622963	70.955329
805.505895	43.780035	70.960334
804.783780	40.790169	70.965338
803.701257	50.222229	70.970343
803.231686	32.724013	70.975348
802.740378	39.518397	70.980353
802.358729	32.106295	70.985358
801.283842	32.468330	70.990362
800.647471	36.712291	70.995367
800.110384	40.000610	71.000372
799.778943	35.584527	71.005377
799.062640	34.952795	71.010382
798.399684	41.200511	71.015386
797.402773	38.342700	71.020391
796.547885	29.067916	71.025396
795.431295	34.630929	71.030401
795.535317	30.055642	71.035406
794.839192	45.822132	71.040410
794.515445	43.357038	71.045415
793.804986	35.147328	71.050420
793.001399	45.758665	71.055425
792.145159	29.928884	71.060430
791.091739	39.884573	71.065434
790.372832	32.150860	71.070439
790.481198	39.515235	71.075444
789.827650	40.218619	71.080449
789.158822	43.080070	71.085454
788.217292	44.113144	71.090458
787.725249	44.691472	71.095463
786.937094	46.797659	71.100468
785.759591	39.785061	71.105473
785.298805	36.247411	71.110478
785.064592	52.550638	71.115482
784.411270	45.541319	71.120487
783.412801	37.790612	71.125492
782.305609	49.038474	71.130497
782.262969	35.698416	71.135502
782.085848	44.554267	71.140506
781.180787	43.514209	71.145511
780.316600	36.134777	71.150516
779.585731	60.198205	71.155521
779.122203	38.614829	71.160526
778.292139	36.367536	71.165530
777.098789	58.419915	71.170535
777.038433	31.166447	71.175540
776.483982	42.379924	71.180545
775.719342	36.127905	71.185550
774.874050	43.399684	71.190554
774.271558	37.255888	71.195559
773.814784	36.344732	71.200564
772.771618	47.035216	71.205569
771.941995	45.413887	71.210574
771.583381	42.754080	71.215578
771.213355	48.742286	71.220583
770.803689	41.925988	71.225588
769.451483	46.652919	71.230593
768.827947	44.027405	71.235598
768.262613	34.730185	71.240602
767.775806	48.479606	71.245607
767.086399	33.287153	71.250612
766.344400	52.090197	71.255617
766.149723	34.474114	71.260622
765.260234	43.347186	71.265626
764.371656	43.438308	71.270631
763.871138	45.875589	71.275636
763.147524	41.788446	71.280641
762.096623	45.798800	71.285646
761.389251	44.285741	71.290650
760.864513	40.214244	71.295655
760.701162	44.300907	71.300660
760.063422	53.378327	71.305665
759.384721	39.313235	71.310670
758.637190	40.629238	71.315674
757.968917	46.587659	71.320679
757.256205	47.024511	71.325684
756.719375	41.540452	71.330689
756.032002	40.640782	71.335694
754.903660	44.756506	71.340698
754.178231	37.320301	71.345703
753.822101	33.438000	71.350708
753.369286	42.686239	71.355713
752.566682	34.883865	71.360718
751.755112	36.966981	71.365722
751.093410	39.194966	71.370727
750.918511	33.631211	71.375732
749.971539	44.549228	71.380737
749.066578	32.571729	71.385742
748.311445	34.379363	71.390746
748.149241	29.341853	71.395751
747.471669	32.181051	71.400756
746.057762	39.374637	71.405761
746.013702	26.971503	71.410766
745.297344	36.731617	71.415770
744.643502	40.681914	71.420775
743.610916	29.506886	71.425780
743.173508	43.861856	71.430785
742.093323	41.853088	71.435790
741.905368	33.862973	71.440794
741.620056	42.501089	71.445799
740.897986	28.848185	71.450804
739.870458	44.626445	71.455809
739.812042	35.458253	71.460814
738.820613	34.829344	71.465818
737.720755	35.517071	71.470823
737.552144	24.155607	71.475828
736.747555	42.963877	71.480833
735.906642	42.732038	71.485838
735.313977	38.016946	71.490842
734.568500	41.360533	71.495847
734.417979	26.057071	71.500852
733.341585	43.103059	71.505857
732.488564	39.025493	71.510862
732.292199	36.391899	71.515866
731.710968	40.303829	71.520871
730.702969	41.413737	71.525876
729.901048	42.657986	71.530881
729.318607	37.307351	71.535886
728.878339	37.544718	71.540890
727.841674	36.438905	71.545895
727.571764	41.539141	71.550900
726.784155	38.411499	71.555905
726.106292	38.150548	71.560910
725.279287	41.639579	71.565914
724.461182	37.822954	71.570919
724.456653	40.846724	71.575924
723.665344	45.823405	71.580929
722.796061	36.848977	71.585934
721.679660	45.515347	71.590938
721.351289	36.741791	71.595943
720.965058	35.392072	71.600948
719.899317	43.865877	71.605953
719.252395	36.281572	71.610958
718.684369	49.898852	71.615962
718.319060	36.611757	71.620967
717.985038	45.055786	71.625972
716.901410	37.459016	71.630977
716.445292	45.723796	71.635982
716.081544	32.551571	71.640986
714.659103	42.061433	71.645991
714.289678	31.324861	71.650996
713.418462	51.294895	71.656001
712.908748	35.853084	71.661006
712.150939	48.194903	71.666010
711.340396	39.214279	71.671015
711.218079	36.770741	71.676020
710.160875	36.128663	71.681025
709.411811	36.476702	71.686030
708.634777	36.004473	71.691034
708.434300	35.951357	71.696039
708.100509	40.377387	71.701044
706.701732	47.489742	71.706049
706.184623	37.120449	71.711054
705.902174	34.126838	71.716058
705.057010	38.159645	71.721063
704.127074	34.859138	71.726068
703.578842	46.972049	71.731073
703.164206	50.471119	71.736078
702.571482	39.891521	71.741082
701.573455	49.676003	71.746087
700.770441	35.558196	71.751092
700.287215	41.775735	71.756097
700.008742	42.651223	71.761102
698.782116	44.565487	71.766106
697.900253	42.553545	71.771111
697.604192	40.460939	71.776116
697.464402	38.589448	71.781121
696.496978	37.857388	71.786126
695.802225	30.091481	71.791130
694.942653	38.770576	71.796135
694.881154	38.007799	71.801140
693.504438	48.931188	71.806145
692.923974	42.058530	71.811150
692.923484	42.667410	71.816154
691.323964	39.430952	71.821159
690.749396	42.154419	71.826164
690.333522	47.586975	71.831169
689.910152	40.928993	71.836174
689.424733	38.185318	71.841178
688.273964	43.801125	71.846183
687.766237	41.540381	71.851188
687.029769	56.318289	71.856193
686.746094	36.729491	71.861198
685.515286	47.632802	71.866202
685.066024	50.605969	71.871207
684.809426	45.539339	71.876212
684.157148	41.390402	71.881217
683.451091	43.444122	71.886222
682.626844	45.617586	71.891226
681.899128	48.409596	71.896231
681.018266	40.111946	71.901236
679.918111	51.838102	71.906241
679.704764	39.260080	71.911246
679.255228	42.679555	71.916250
678.812048	46.342439	71.921255
677.948166	43.203306	71.926260
677.045963	35.191325	71.931265
676.981971	36.985112	71.936270
675.903211	32.386868	71.941274
675.055303	40.862268	71.946279
674.733565	30.854528	71.951284
674.038200	41.464422	71.956289
673.082757	37.644456	71.961294
672.596927	33.147330	71.966298
672.021274	41.338109	71.971303
671.871649	40.833787	71.976308
670.552230	45.512969	71.981313
669.663927	41.198200	71.986318
669.531583	50.302381	71.991322
668.700530	43.173176	71.996327
667.781925	34.192436	72.001332
667.169906	44.450026	72.006337
667.237827	33.959200	72.011342
665.933709	29.100391	72.016346
664.707690	44.139170	72.021351
664.467922	35.845090	72.026356
663.796103	36.773759	72.031361
663.522763	32.454103	72.036366
663.266750	36.437254	72.041370
662.230250	38.314950	72.046375
662.058532	34.280300	72.051380
660.446727	42.809546	72.056385
659.873967	26.952040	72.061390
659.229019	35.327312	72.066394
658.840442	32.866257	72.071399
658.503243	31.535548	72.076404
657.350521	38.041052	72.081409
656.605531	22.791281	72.086414
656.495316	30.467978	72.091418
655.276642	29.572526	72.096423
654.800883	39.529302	72.101428
654.088029	24.968251	72.106433
653.605306	34.377370	72.111438
652.469363	19.224556	72.116442
651.778546	29.286534	72.121447
651.775678	26.095450	72.126452
651.091006	29.318989	72.131457
650.164142	25.633252	72.136462
649.334035	18.486571	72.141466
648.779323	24.710763	72.146471
648.548695	27.289578	72.151476
647.262736	32.207858	72.156481
646.679018	25.636930	72.161486
646.101232	29.822707	72.166490
645.764805	34.774270	72.171495
644.981365	33.461013	72.176500
643.819181	34.735854	72.181505
643.480728	29.195008	72.186510
643.278656	23.067912	72.191514
641.871043	31.014303	72.196519
641.299637	29.265170	72.201524
640.615622	26.639865	72.206529
640.490235	30.179602	72.211534
639.873453	35.502234	72.216538
638.597056	39.628967	72.221543
638.319846	25.213003	72.226548
637.920457	39.226034	72.231553
636.957289	35.162893	72.236558
636.018980	21.822016	72.241562
635.354403	42.837742	72.246567
635.368780	28.323300	72.251572
634.391835	36.525953	72.256577
633.546894	28.563222	72.261582
633.029171	33.127355	72.266586
631.866095	39.612442	72.271591
632.159549	27.893564	72.276596
631.397604	31.145184	72.281601
630.892442	26.559689	72.286606
629.868230	27.470374	72.291610
628.632104	37.344826	72.296615
628.231859	29.257659	72.301620
627.816384	31.910069	72.306625
627.272212	39.570730	72.311630
625.913602	41.375165	72.316634
625.339820	30.992852	72.321639
625.149386	28.247943	72.326644
624.710244	34.698157	72.331649
623.558360	28.036378	72.336654
623.295627	29.976931	72.341658
622.235384	34.988582	72.346663
621.623951	33.565939	72.351668
620.813124	32.017363	72.356673
620.161429	39.796072	72.361678
619.983514	25.495181	72.366682
619.379123	38.090108	72.371687
618.633389	21.823370	72.376692
617.609294	48.604759	72.381697
617.142298	40.548719	72.386702
616.953778	34.922497	72.391706
615.677620	34.083527	72.396711
615.118939	26.792704	72.401716
614.400919	36.419070	72.406721
613.825132	22.982620	72.411726
613.136734	29.677529	72.416730
612.661979	32.169076	72.421735
612.145200	28.022238	72.426740
611.014809	37.067751	72.431745
610.141890	33.479090	72.436750
609.770486	26.185249	72.441754
609.225172	31.985343	72.446759
608.896903	34.584444	72.451764
607.654563	36.897057	72.456769
607.322746	25.140578	72.461774
606.959548	33.795826	72.466778
605.677928	25.341279	72.471783
605.138529	25.905107	72.476788
604.647402	29.809016	72.481793
604.133607	27.355301	72.486798
603.171063	28.883783	72.491802
602.296339	30.574891	72.496807
601.665030	26.102533	72.501812
601.191837	37.389810	72.506817
600.802328	26.729009	72.511822
600.200177	32.358389	72.516826
599.314764	36.708288	72.521831
598.789936	18.933548	72.526836
597.770156	34.467753	72.531841
597.023164	21.525343	72.536846
596.881928	31.871948	72.541850
596.097110	34.313538	72.546855
595.218126	36.361709	72.551860
594.576731	36.121794	72.556865
593.901500	25.481272	72.561870
593.696609	23.741582	72.566874
592.452237	31.813379	72.571879
591.944932	25.764868	72.576884
591.239913	25.744816	72.581889
590.898148	45.159034	72.586894
590.519193	21.020322	72.591898
589.497172	38.811440	72.596903
589.100347	25.721796	72.601908
587.672100	33.721962	72.606913
587.144779	23.496265	72.611918
586.702962	25.553652	72.616922
585.950277	38.596389	72.621927
585.655176	30.492485	72.626932
584.531517	45.707370	72.631937
584.069472	31.560545	72.636942
583.413075	33.164847	72.641946
582.997832	31.975886	72.646951
582.184504	27.172990	72.651956
581.097751	39.541987	72.656961
580.846542	30.316220	72.661966
580.570694	31.289070	72.666970
579.412261	42.526231	72.671975
579.031548	35.900907	72.676980
578.276126	29.724766	72.681985
577.524867	39.446318	72.686990
576.582867	31.100112	72.691994
575.892428	37.476822	72.696999
575.919872	22.892507	72.702004
575.107242	36.827859	72.707009
573.986599	25.408340	72.712014
573.510579	33.725180	72.717018
572.734945	38.489673	72.722023
572.575808	24.201573	72.727028
571.342106	39.832941	72.732033
570.439303	35.055337	72.737038
570.014812	35.608754	72.742042
569.385101	37.577805	72.747047
568.871318	31.613905	72.752052
568.169453	28.231397	72.757057
567.323709	28.287382	72.762062
567.194663	26.374769	72.767066
566.404366	28.749433	72.772071
565.555008	26.897940	72.777076
564.850393	41.274972	72.782081
564.599970	37.069947	72.787086
563.797548	29.475776	72.792090
562.704938	26.283240	72.797095
562.270729	23.100944	72.802100
561.672315	30.729250	72.807105
561.105991	23.032822	72.812110
560.088779	32.640623	72.817114
559.255142	34.159627	72.822119
559.217585	25.577904	72.827124
558.684333	41.772619	72.832129
557.840329	34.350646	72.837134
557.271827	36.144375	72.842138
556.278864	37.415954	72.847143
555.865487	34.760179	72.852148
554.502056	37.566754	72.857153
554.231819	41.217874	72.862158
553.866002	31.862139	72.867162
552.848667	40.506478	72.872167
552.588206	31.816761	72.877172
551.764939	36.188313	72.882177
551.483092	32.779903	72.887182
550.631804	42.627780	72.892186
549.490674	37.900763	72.897191
549.412739	30.087116	72.902196
548.494325	36.859681	72.907201
547.551568	32.436948	72.912206
547.041565	35.668959	72.917210
546.416232	38.566115	72.922215
546.249500	29.672242	72.927220
544.967678	38.435981	72.932225
544.383351	34.700453	72.937230
543.904939	30.771440	72.942234
542.911491	42.791284	72.947239
542.372049	31.473155	72.952244
541.468740	30.226335	72.957249
541.281275	28.097532	72.962254
540.866514	33.774342	72.967258
539.834069	40.803188	72.972263
539.021445	26.701190	72.977268
538.456744	32.720420	72.982273
538.252918	38.127095	72.987278
537.039726	37.953050	72.992282
536.133752	40.798723	72.997287
536.229106	28.105338	73.002292
535.589642	38.928691	73.007297
534.681432	36.547282	73.012302
533.851232	33.096921	73.017306
533.182115	35.854402	73.022311
532.782601	30.794798	73.027316
531.758549	38.763721	73.032321
531.005085	31.259531	73.037326
530.989568	28.748534	73.042330
530.141458	38.909711	73.047335
529.016561	33.276554	73.052340
528.500065	24.261791	73.057345
527.897252	35.084034	73.062350
527.549016	27.554717	73.067354
526.487734	43.913973	73.072359
526.009563	33.554307	73.077364
525.575514	42.638731	73.082369
524.474218	45.684253	73.087374
523.727538	37.825755	73.092378
522.910860	42.344496	73.097383
522.868418	26.389950	73.102388
522.207340	44.170896	73.107393
521.352494	33.803431	73.112398
520.738912	35.102893	73.117402
520.250078	44.628118	73.122407
519.610001	33.073723	73.127412
518.374245	36.525430	73.132417
517.738561	38.052335	73.137422
517.501345	36.160110	73.142426
516.888114	36.954908	73.147431
516.118809	32.625979	73.152436
515.219125	38.482543	73.157441
514.806422	32.534093	73.162446
514.568984	28.520969	73.167450
513.306489	34.345447	73.172455
512.879012	34.766889	73.177460
512.094719	27.296004	73.182465
511.183995	35.128610	73.187470
510.635811	29.857737	73.192474
509.677995	38.798526	73.197479
509.555928	33.794072	73.202484
509.219551	34.254616	73.207489
508.220228	35.842608	73.212494
507.692406	29.321162	73.217498
506.878431	42.217566	73.222503
506.245806	29.331084	73.227508
505.353606	35.041382	73.232513
504.917991	41.669241	73.237518
504.382093	31.380279	73.242522
503.332822	32.282392	73.247527
502.762245	38.804021	73.252532
502.298806	34.601404	73.257537
501.934751	33.888412	73.262542
500.755789	40.278314	73.267546
500.187924	40.242745	73.272551
499.624993	45.060103	73.277556
498.645714	33.640176	73.282561
497.872502	35.390840	73.287566
497.411739	27.160388	73.292570
496.723356	32.268956	73.297575
496.864646	34.980913	73.302580
495.556921	41.801326	73.307585
494.976478	31.276621	73.312590
494.432739	29.232966	73.317594
493.846967	34.184843	73.322599
493.070539	23.595176	73.327604
492.271524	28.749753	73.332609
491.306822	34.764911	73.337614
491.125554	19.657216	73.342618
490.004218	38.706776	73.347623
489.485127	33.855460	73.352628
488.740101	33.649428	73.357633
488.738280	30.114417	73.362638
487.914124	26.568498	73.367642
486.868131	33.791900	73.372647
486.971017	28.124003	73.377652
485.873155	31.377142	73.382657
484.819410	35.582011	73.387662
484.189828	30.568534	73.392666
483.828625	36.700428	73.397671
482.802793	26.981526	73.402676
482.011014	36.051982	73.407681
481.529726	29.426938	73.412686
481.278572	33.964395	73.417690
480.563601	27.725078	73.422695
479.660135	37.209131	73.427700
479.196052	37.801986	73.432705
478.605140	38.318857	73.437710
477.758028	22.822097	73.442714
477.066876	31.047069	73.447719
476.571895	40.267355	73.452724
475.749279	30.804651	73.457729
474.587021	25.790893	73.462734
474.121911	29.198683	73.467738
473.274732	44.653391	73.472743
473.164972	28.447811	73.477748
472.737404	35.362961	73.482753
472.059152	27.779006	73.487758
471.509821	26.955194	73.492762
470.826858	35.144172	73.497767
469.958669	33.174292	73.502772
468.815715	32.258984	73.507777
468.568244	43.573388	73.512782
467.828061	30.044912	73.517786
466.996725	32.645333	73.522791
466.304187	31.964183	73.527796
465.853378	31.000099	73.532801
465.339581	35.521058	73.537806
464.808988	39.618930	73.542810
463.930858	33.055540	73.547815
463.413052	32.573625	73.552820
463.046021	32.834062	73.557825
461.817291	33.824708	73.562830
461.543106	32.651140	73.567834
460.716089	43.553273	73.572839
459.581041	32.009957	73.577844
459.031908	32.196911	73.582849
458.157775	35.652528	73.587854
458.170059	30.462676	73.592858
457.444246	44.537183	73.597863
456.388360	30.145985	73.602868
455.973908	41.911180	73.607873
455.280887	37.120699	73.612878
454.714966	31.969358	73.617882
453.754457	41.897735	73.622887
453.093333	34.383592	73.627892
452.325292	41.020268	73.632897
452.221655	38.975883	73.637902
451.963860	31.479478	73.642906
450.521845	45.303836	73.647911
450.057842	33.609452	73.652916
449.407467	29.548595	73.657921
448.594315	45.428380	73.662926
447.917229	23.945426	73.667930
447.263090	40.389631	73.672935
447.195380	27.036285	73.677940
446.257305	32.626181	73.682945
445.380372	36.754009	73.687950
445.160007	29.239027	73.692954
443.914037	41.817933	73.697959
443.173623	28.850884	73.702964
442.726120	32.851943	73.707969
442.198734	28.530225	73.712974
441.809541	23.033775	73.717978
440.020543	30.544307	73.722983
440.153270	27.658043	73.727988
439.639132	34.077650	73.732993
438.843150	26.496697	73.737998
438.058469	15.350153	73.743002
437.251673	30.326924	73.748007
436.503439	16.946409	73.753012
436.544225	28.933937	73.758017
435.426620	30.698494	73.763022
434.828144	22.027973	73.768026
434.163581	30.955168	73.773031
433.976091	30.326013	73.778036
432.854261	27.439383	73.783041
432.354118	36.103847	73.788046
431.521471	22.545974	73.793050
430.177514	42.116711	73.798055
430.030669	25.492867	73.803060
429.480478	34.859141	73.808065
429.048928	35.699126	73.813070
428.857011	43.021421	73.818074
427.412765	38.429495	73.823079
427.003178	38.029689	73.828084
426.273253	25.329052	73.833089
425.330904	33.920480	73.838094
424.812738	30.516631	73.843098
424.319884	38.036681	73.848103
423.616890	30.130266	73.853108
422.972876	43.729711	73.858113
422.175565	23.530603	73.863118
422.057509	32.283988	73.868122
421.341080	42.288596	73.873127
419.993460	24.449494	73.878132
419.694442	30.238755	73.883137
418.749474	34.244972	73.888142
418.617553	22.128698	73.893146
417.346148	31.740777	73.898151
416.999337	24.960287	73.903156
416.355722	31.843637	73.908161
415.570485	38.987669	73.913166
414.899436	24.629794	73.918170
413.862656	47.087785	73.923175
413.590727	29.097774	73.928180
413.402391	39.648992	73.933185
412.132353	30.019500	73.938190
411.523896	34.169210	73.943194
411.049753	39.278352	73.948199
410.867167	28.806972	73.953204
409.806477	35.808823	73.958209
408.884394	47.125074	73.963214
408.532113	40.044262	73.968218
407.843251	36.718077	73.973223
406.774182	25.661009	73.978228
406.355827	39.875753	73.983233
405.701437	33.603153	73.988238
405.300285	27.914655	73.993242
404.333536	36.751245	73.998247
403.562709	33.252048	74.003252
403.126715	32.332923	74.008257
402.428697	41.689647	74.013262
402.350705	25.482178	74.018266
401.179880	34.420670	74.023271
400.649195	19.338717	74.028276
399.757416	30.404133	74.033281
398.709906	24.960558	74.038286
398.272141	24.284559	74.043290
397.482560	34.475858	74.048295
397.309682	19.176045	74.053300
397.148638	29.051145	74.058305
395.619368	35.577333	74.063310
395.220281	21.881005	74.068314
394.876392	28.003835	74.073319
394.029756	29.843497	74.078324
393.047684	34.926352	74.083329
392.566837	26.894666	74.088334
391.990354	28.300206	74.093338
390.960461	34.433014	74.098343
390.355086	30.363426	74.103348
389.790431	22.483866	74.108353
389.515130	33.078898	74.113358
389.034603	27.043520	74.118362
387.669596	38.513929	74.123367
387.106775	32.797582	74.128372
386.768859	31.132725	74.133377
385.777342	41.986972	74.138382
385.416788	27.831930	74.143386
384.728358	36.348215	74.148391
384.053782	22.648484	74.153396
383.288305	35.852557	74.158401
382.504354	32.721301	74.163406
382.263269	34.596927	74.168410
381.578876	35.789439	74.173415
380.655556	30.803881	74.178420
380.420353	23.772232	74.183425
379.218445	30.842327	74.188430
378.451492	31.546541	74.193434
377.566196	35.477033	74.198439
377.408904	24.925940	74.203444
376.890755	32.863173	74.208449
376.093466	36.453222	74.213454
375.386607	24.942647	74.218458
374.889371	31.988751	74.223463
374.085133	30.119099	74.228468
373.033478	21.412014	74.233473
372.455527	32.558308	74.238478
372.209202	20.236355	74.243482
371.365157	36.838556	74.248487
371.060042	34.790017	74.253492
370.389428	25.044528	74.258497
369.410445	30.636236	74.263502
368.720129	31.052283	74.268506
367.640869	32.222574	74.273511
367.218359	35.677208	74.278516
366.885285	29.216225	74.283521
365.911320	42.018308	74.288526
365.995128	22.027308	74.293530
364.807626	33.324360	74.298535
364.195938	34.076372	74.303540
363.870686	19.469456	74.308545
362.537967	41.507848	74.313550
362.000133	28.877546	74.318554
361.557899	33.924839	74.323559
361.101303	25.029887	74.328564
359.862008	33.605581	74.333569
359.292104	30.183187	74.338574
359.148572	22.211292	74.343578
358.210570	39.706806	74.348583
357.527999	22.321565	74.353588
356.751190	31.993613	74.358593
356.009946	27.185623	74.363598
355.769347	28.395720	74.368602
354.919634	30.350999	74.373607
354.115701	25.740653	74.378612
353.806849	20.795949	74.383617
353.250348	31.577715	74.388622
352.335113	24.492028	74.393626
351.291597	30.800478	74.398631
350.909389	22.514975	74.403636
350.801011	33.931776	74.408641
349.568653	27.216740	74.413646
349.073260	31.616516	74.418650
348.368777	35.193359	74.423655
347.465040	26.740244	74.428660
346.608390	34.362435	74.433665
345.990658	32.089343	74.438670
345.717205	28.938239	74.443674
345.393831	34.947423	74.448679
344.763497	30.848712	74.453684
343.835526	33.298998	74.458689
343.067432	27.424577	74.463694
342.343515	34.642428	74.468698
341.453386	36.410194	74.473703
341.026426	25.805894	74.478708
340.885346	33.845456	74.483713
339.834553	42.700193	74.488718
339.192235	30.945960	74.493722
338.261418	31.613228	74.498727
337.195540	27.654896	74.503732
336.493079	30.723657	74.508737
335.959770	37.250410	74.513742
335.845265	28.422363	74.518746
334.980939	35.478096	74.523751
335.067980	25.335909	74.528756
333.822333	34.054547	74.533761
332.674322	32.726961	74.538766
332.965609	36.865746	74.543770
331.909882	33.594904	74.548775
331.174791	31.983895	74.553780
330.380858	38.290423	74.558785
330.076275	33.117965	74.563790
329.110698	27.462675	74.568794
328.164351	35.764619	74.573799
327.944144	29.542691	74.578804
327.490141	27.975190	74.583809
326.606256	29.051283	74.588814
325.992560	28.188879	74.593818
325.378056	23.633506	74.598823
324.516992	32.003855	74.603828
323.869867	25.186098	74.608833
323.224369	36.833581	74.613838
322.809813	21.064541	74.618842
321.402615	37.173056	74.623847
320.696872	14.570418	74.628852
320.361638	25.100881	74.633857
319.939734	40.174025	74.638862
319.574629	25.808426	74.643866
318.529606	43.404584	74.648871
318.156387	21.646194	74.653876
317.526760	30.211460	74.658881
316.112934	31.830900	74.663886
315.753632	35.767459	74.668890
315.023872	32.370555	74.673895
314.788387	28.407608	74.678900
314.494207	25.989919	74.683905
313.224723	35.423547	74.688910
312.720993	20.660595	74.693914
311.994233	37.357648	74.698919
310.950276	21.428743	74.703924
310.170753	27.009177	74.708929
309.650665	27.200995	74.713934
309.400924	28.852508	74.718938
308.612516	31.908168	74.723943
308.531673	28.731101	74.728948
307.424152	24.232238	74.733953
306.767276	36.009266	74.738958
306.337924	26.737838	74.743962
305.016273	35.334566	74.748967
304.265960	26.246757	74.753972
303.900653	38.098735	74.758977
303.464116	28.653416	74.763982
303.206079	29.355381	74.768986
301.854373	33.077974	74.773991
301.551364	33.006543	74.778996
301.418857	23.195811	74.784001
299.957087	27.569859	74.789006
299.314840	22.159506	74.794010
298.749490	25.770950	74.799015
298.045253	30.609285	74.804020
297.224215	31.519258	74.809025
296.587065	34.404160	74.814030
296.359000	37.709542	74.819034
295.522769	27.197298	74.824039
294.822719	29.409428	74.829044
294.299114	42.404663	74.834049
293.521310	30.760351	74.839054
292.889255	28.413866	74.844058
292.131495	36.867104	74.849063
291.578616	30.242484	74.854068
290.855699	28.985928	74.859073
289.816944	23.889506	74.864078
289.456414	32.254194	74.869082
288.561594	34.286069	74.874087
288.384038	18.919221	74.879092
287.771861	20.947040	74.884097
286.697396	37.999131	74.889102
286.562202	27.362532	74.894106
285.565399	41.201143	74.899111
284.741289	32.115640	74.904116
284.035042	32.728208	74.909121
283.472946	31.507519	74.914126
283.146593	27.492832	74.919130
282.408598	39.306449	74.924135
281.339253	38.822606	74.929140
281.103562	30.341878	74.934145
280.590458	41.044204	74.939150
279.714883	31.233649	74.944154
278.805849	30.290606	74.949159
278.204993	32.458545	74.954164
277.813166	31.690092	74.959169
276.543898	35.175638	74.964174
276.140300	21.487952	74.969178
275.372339	33.236958	74.974183
275.368967	24.681357	74.979188
274.555584	30.200969	74.984193
273.353283	31.933367	74.989198
273.176504	26.496130	74.994202
272.431860	31.241567	74.999207
271.384942	33.811761	75.004212
270.842333	36.367796	75.009217
270.181661	25.868579	75.014222
269.790425	27.932145	75.019226
269.039171	31.648921	75.024231
267.963173	27.875156	75.029236
267.714993	28.510901	75.034241
267.335570	32.371826	75.039246
266.931309	24.654388	75.044250
265.810529	28.471069	75.049255
265.024190	30.014165	75.054260
264.685059	31.895967	75.059265
263.251333	37.454550	75.064270
262.968704	23.861119	75.069274
262.477123	32.817537	75.074279
262.121931	28.283921	75.079284
261.177669	27.997759	75.084289
260.415740	30.738562	75.089294
260.400405	31.696724	75.094298
258.854355	31.582185	75.099303
257.942609	16.512151	75.104308
257.760357	29.241657	75.109313
256.925069	32.437264	75.114318
256.849540	22.486574	75.119322
255.981797	36.727224	75.124327
255.038864	30.803438	75.129332
254.851141	32.143882	75.134337
253.495863	29.723470	75.139342
252.773969	34.613515	75.144346
252.097861	30.418053	75.149351
251.756199	22.651218	75.154356
251.584249	35.776466	75.159361
250.870337	31.049308	75.164366
250.252034	30.320118	75.169370
249.514822	37.532224	75.174375
248.475529	30.054788	75.179380
247.764714	26.811001	75.184385
246.813190	33.992618	75.189390
246.766461	21.011270	75.194394
246.286857	38.973027	75.199399
245.285664	34.085094	75.204404
244.264498	27.486257	75.209409
243.917660	34.975165	75.214414
243.678844	30.102889	75.219418
242.159219	33.301943	75.224423
241.596066	27.801729	75.229428
241.311000	33.967233	75.234433
240.910511	44.027160	75.239438
240.174944	34.064996	75.244442
239.126966	34.937052	75.249447
238.780313	24.944433	75.254452
238.239470	28.717557	75.259457
236.950003	35.090489	75.264462
236.556388	31.066032	75.269466
236.090600	31.840547	75.274471
235.580699	26.880606	75.279476
234.883826	33.368795	75.284481
233.987508	40.689847	75.289486
233.841968	26.133158	75.294490
232.426644	36.298097	75.299495
231.623079	35.951671	75.304500
231.212989	34.772990	75.309505
230.546215	35.052863	75.314510
230.489117	31.643365	75.319514
229.327334	39.013046	75.324519
228.555398	42.433522	75.329524
228.086563	30.645369	75.334529
227.502728	33.204831	75.339534
227.142038	30.996445	75.344538
226.225107	35.187486	75.349543
225.745477	41.000825	75.354548
224.600426	30.460576	75.359553
223.548074	36.918711	75.364558
223.295420	26.010700	75.369562
222.902922	25.275480	75.374567
222.687571	35.337424	75.379572
221.943667	36.932114	75.384577
220.935170	40.931182	75.389582
220.129584	33.913222	75.394586
219.039248	32.790955	75.399591
218.299089	34.891233	75.404596
218.206508	27.447380	75.409601
217.835326	37.485286	75.414606
217.512582	25.788962	75.419610
216.402493	31.261280	75.424615
215.647974	31.772757	75.429620
214.553610	31.890577	75.434625
213.762415	38.794342	75.439630
213.706643	30.926741	75.444634
213.056492	38.131283	75.449639
212.519662	34.754116	75.454644
211.401362	21.983035	75.459649
210.570061	34.339797	75.464654
210.355435	22.424398	75.469658
209.836617	33.586513	75.474663
209.070752	29.209840	75.479668
208.636554	37.609935	75.484673
207.552585	38.052518	75.489678
206.592534	30.305434	75.494682
205.930986	38.842698	75.499687
205.333617	39.920461	75.504692
204.954867	29.504048	75.509697
204.487969	37.048370	75.514702
203.795706	30.650995	75.519706
203.131329	39.806855	75.524711
202.585098	33.518656	75.529716
201.731123	29.892445	75.534721
200.565367	38.745055	75.539726
200.117447	36.003397	75.544730
199.734453	33.270311	75.549735
199.247826	35.073138	75.554740
198.405228	27.769365	75.559745
197.533823	33.377095	75.564750
197.254779	29.329650	75.569754
196.553592	30.364045	75.574759
195.663494	33.569986	75.579764
194.777202	28.561260	75.584769
194.298210	38.496512	75.589774
194.274277	22.982192	75.594778
193.388772	31.550429	75.599783
192.344289	35.069560	75.604788
191.956003	34.240635	75.609793
190.596153	39.729133	75.614798
190.214393	32.709842	75.619802
189.645399	38.859121	75.624807
189.168500	30.896245	75.629812
188.768225	28.572757	75.634817
187.288751	33.375455	75.639822
187.294605	28.065222	75.644826
186.283775	34.770630	75.649831
186.004899	31.735528	75.654836
185.312910	26.300025	75.659841
184.079295	37.361655	75.664846
184.055905	28.407143	75.669850
183.355633	26.930975	75.674855
182.596488	33.509525	75.679860
182.191704	31.901091	75.684865
181.317719	35.432464	75.689870
180.698674	31.404539	75.694874
179.660583	41.375324	75.699879
178.978087	36.362492	75.704884
178.839884	32.920198	75.709889
177.792277	38.887178	75.714894
177.249871	30.652486	75.719898
176.365402	31.675111	75.724903
176.168127	26.755223	75.729908
175.233101	30.621170	75.734913
174.310979	45.682617	75.739918
173.881172	25.469200	75.744922
173.516937	27.626241	75.749927
172.331499	26.104436	75.754932
171.932202	22.377358	75.759937
171.171519	25.237831	75.764942
170.888345	27.533329	75.769946
169.941941	24.106366	75.774951
169.012728	32.754117	75.779956
168.776378	32.960646	75.784961
168.052987	34.671925	75.789966
167.445866	20.048511	75.794970
166.380600	35.697302	75.799975
166.000259	30.324073	75.804980
165.995751	18.583335	75.809985
164.749644	35.322212	75.814990
163.785849	28.805727	75.819994
163.083379	32.052723	75.824999
162.992943	31.255156	75.830004
161.855874	31.581651	75.835009
161.025654	35.393047	75.840014
160.960536	25.743474	75.845018
160.048516	36.712834	75.850023
159.247894	33.805081	75.855028
158.557901	36.625904	75.860033
157.547713	32.855889	75.865038
157.536604	29.888479	75.870042
157.116281	37.190422	75.875047
156.126405	33.395092	75.880052
155.770094	32.225196	75.885057
154.853532	42.755332	75.890062
154.141564	32.191798	75.895066
153.453721	35.482194	75.900071
152.596611	37.090224	75.905076
152.614315	28.577002	75.910081
151.597888	35.559271	75.915086
150.727261	33.080562	75.920090
150.067972	34.929852	75.925095
149.416431	37.337707	75.930100
148.721480	34.225457	75.935105
147.671359	35.760190	75.940110
147.652152	29.083632	75.945114
147.177018	39.578072	75.950119
146.275266	47.425125	75.955124
145.515873	20.283353	75.960129
144.821669	34.510542	75.965134
144.490011	34.140935	75.970138
143.442219	33.425065	75.975143
142.852034	33.880400	75.980148
142.350402	31.692926	75.985153
141.187513	36.993928	75.990158
140.632068	33.996626	75.995162
139.888130	37.571928	76.000167
139.273830	34.027366	76.005172
139.233403	38.608508	76.010177
138.816880	42.697709	76.015182
137.952474	37.067370	76.020186
137.125902	42.954967	76.025191
136.432592	43.601783	76.030196
135.269848	43.845656	76.035201
134.646592	41.611347	76.040206
134.775567	32.892729	76.045210
133.726981	29.811646	76.050215
132.700144	38.038177	76.055220
132.307419	34.369978	76.060225
131.921129	35.702672	76.065230
130.903348	30.229255	76.070234
130.373335	39.157127	76.075239
129.974915	39.211314	76.080244
129.218815	34.267006	76.085249
128.053699	43.117966	76.090254
127.481899	40.402385	76.095258
127.187247	46.712926	76.100263
126.436274	45.085592	76.105268
125.670053	43.216270	76.110273
124.670131	34.108411	76.115278
124.515342	32.532660	76.120282
124.026029	42.512142	76.125287
123.279990	43.269869	76.130292
122.678118	43.134158	76.135297
121.746222	32.999932	76.140302
120.898266	39.485432	76.145306
120.047454	34.332311	76.150311
119.635583	41.295455	76.155316
119.477946	35.442035	76.160321
118.366418	44.341223	76.165326
117.609742	36.684745	76.170330
117.133105	33.641767	76.175335
116.392829	41.702764	76.180340
116.308767	31.296149	76.185345
115.000553	45.756882	76.190350
114.657650	37.960306	76.195354
113.866714	34.316191	76.200359
112.735258	41.529701	76.205364
112.453718	39.083216	76.210369
111.781355	41.368248	76.215374
111.344607	35.679184	76.220378
110.804046	44.730164	76.225383
109.565646	45.661026	76.230388
109.105730	40.675797	76.235393
108.405252	41.347418	76.240398
108.006840	32.889517	76.245402
106.878082	36.090972	76.250407
106.281699	40.041708	76.255412
105.929283	36.863808	76.260417
105.419797	43.104534	76.265422
104.937243	47.864990	76.270426
104.163891	32.413420	76.275431
103.206171	43.174053	76.280436
102.440477	30.881367	76.285441
101.322654	38.477468	76.290446
100.986740	38.578461	76.295450
100.327586	39.372799	76.300455
99.900453	31.460357	76.305460
99.932386	25.956744	76.310465
98.742037	39.025203	76.315470
98.234703	30.988363	76.320474
97.698155	32.811784	76.325479
96.674771	41.146585	76.330484
95.981941	31.557698	76.335489
95.136243	34.874860	76.340494
94.765532	33.658386	76.345498
93.873580	30.886644	76.350503
93.115511	36.613521	76.355508
92.906203	31.687677	76.360513
92.259610	35.629076	76.365518
91.531267	31.963949	76.370522
90.468594	43.378389	76.375527
90.017682	38.369653	76.380532
89.485720	36.981784	76.385537
88.539598	32.788437	76.390542
88.186658	31.704744	76.395546
87.693017	33.701091	76.400551
86.860624	31.683070	76.405556
86.236274	31.456340	76.410561
85.182387	43.137453	76.415566
84.848608	26.552967	76.420570
84.004105	36.767284	76.425575
83.191199	28.604146	76.430580
83.027166	28.824381	76.435585
82.101064	32.455556	76.440590
81.062805	34.024693	76.445594
80.481716	35.866260	76.450599
80.220809	36.663320	76.455604
80.193727	32.108948	76.460609
78.508334	41.148553	76.465614
78.050440	40.638244	76.470618
77.502362	36.712567	76.475623
77.073141	39.450823	76.480628
76.214563	32.980672	76.485633
75.464745	43.561504	76.490638
75.066924	33.132397	76.495642
74.117077	37.199432	76.500647
73.161481	38.928848	76.505652
72.254066	25.409882	76.510657
71.783987	37.251764	76.515662
71.757702	32.720919	76.520666
71.365260	39.960079	76.525671
70.223303	39.066878	76.530676
69.861414	27.047265	76.535681
69.203985	38.978951	76.540686
68.064379	45.608751	76.545690
67.168915	39.833589	76.550695
66.654370	41.680316	76.555700
66.706382	35.227361	76.560705
65.487523	52.635278	76.565710
64.780516	42.667049	76.570714
64.199247	39.976648	76.575719
63.774204	38.907611	76.580724
63.293872	42.989653	76.585729
62.117467	44.030494	76.590734
61.695240	38.703388	76.595738
61.491582	38.808522	76.600743
60.224265	40.034169	76.605748
59.516821	34.457675	76.610753
58.678006	43.669766	76.615758
58.529497	35.156251	76.620762
57.668647	29.856529	76.625767
56.562419	42.572557	76.630772
56.288937	30.556190	76.635777
55.616750	42.838729	76.640782
55.623487	30.045990	76.645786
54.647593	40.623459	76.650791
53.783949	43.282778	76.655796
53.189544	39.686183	76.660801
52.140601	36.907957	76.665806
51.613541	28.325518	76.670810
51.119401	38.655845	76.675815
50.592422	33.643484	76.680820
49.548138	33.663507	76.685825
48.787962	33.143070	76.690830
48.624816	36.997910	76.695834
48.104660	30.259338	76.700839
47.077771	32.205131	76.705844
46.661101	41.871846	76.710849
46.117566	37.404578	76.715854
45.182151	42.030698	76.720858
44.170122	35.006314	76.725863
43.403639	36.719770	76.730868
43.362350	34.052056	76.735873
42.594157	40.821314	76.740878
41.843967	28.917255	76.745882
41.166214	30.091452	76.750887
40.529786	41.124118	76.755892
40.008773	25.908296	76.760897
39.185909	47.988470	76.765902
38.891189	30.133094	76.770906
37.991303	36.275251	76.775911
36.509828	39.309076	76.780916
36.376208	31.610023	76.785921
35.904152	40.500279	76.790926
35.429398	47.337851	76.795930
34.329231	37.642074	76.800935
33.734400	37.282920	76.805940
33.387121	30.303898	76.810945
32.758343	46.996403	76.815950
32.281372	41.245964	76.820954
31.496745	36.167474	76.825959
30.325456	43.398408	76.830964
29.822617	32.640724	76.835969
28.735382	31.671009	76.840974
28.267444	26.993002	76.845978
27.881758	31.558247	76.850983
27.444124	42.376288	76.855988
27.179840	30.028891	76.860993
26.199031	42.232931	76.865998
25.601933	30.626146	76.871002
24.772413	39.592342	76.876007
23.566902	37.362632	76.881012
23.011772	32.189195	76.886017
22.498855	31.831171	76.891022
22.583243	24.195118	76.896026
21.340737	33.837444	76.901031
20.473831	42.998834	76.906036
20.375316	33.717287	76.911041
19.403868	37.953361	76.916046
18.544961	28.873528	76.921050
17.937735	40.035574	76.926055
17.492592	36.492450	76.931060
17.162110	26.233965	76.936065
15.660382	40.660944	76.941070
15.202618	31.692160	76.946074
15.249994	27.323029	76.951079
14.290355	35.829028	76.956084
13.232886	28.021887	76.961089
12.378319	36.988926	76.966094
12.168243	28.513627	76.971098
11.693280	30.887039	76.976103
10.515726	28.230270	76.981108
10.388837	28.796232	76.986113
9.675922	36.830809	76.991118
8.697066	29.082090	76.996122
7.993842	28.587274	77.001127
7.333004	31.412945	77.006132
7.263885	29.180165	77.011137
6.297041	38.868412	77.016142
5.174474	21.736444	77.021147
4.766134	31.259906	77.026151
4.443536	36.119433	77.031156
3.698050	23.563388	77.036161