Mon Mar 08 18:18:24 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.008842	100.059621	0.000000
-1.420619	86.426852	0.005005
-1.865213	57.440332	0.010010
-3.707488	5.956919	0.015014
-7.083471	-36.183028	0.020019
-12.367229	-37.349072	0.025024
-18.025707	-30.285475	0.030029
-22.805677	-26.790153	0.035034
-26.969298	-20.192055	0.040038
-30.589956	-22.151610	0.045043
-34.216800	-20.724593	0.050048
-38.128403	-22.246657	0.055053
-41.438683	-36.143869	0.060058
-45.616729	-22.747052	0.065062
-49.108644	-28.735568	0.070067
-52.609039	-32.778420	0.075072
-56.460011	-21.002765	0.080077
-60.164800	-28.034320	0.085082
-64.168913	-31.804417	0.090086
-68.072426	-25.815428	0.095091
-71.497989	-29.562699	0.100096
-75.342650	-33.870703	0.105101
-79.021472	-25.435522	0.110106
-82.800281	-31.010801	0.115110
-86.325473	-32.925579	0.120115
-90.416466	-37.591633	0.125120
-94.362223	-30.211359	0.130125
-97.673847	-42.357919	0.135130
-101.523854	-23.896356	0.140134
-105.293595	-25.045146	0.145139
-109.510061	-30.091680	0.150144
-113.209507	-15.938514	0.155149
-116.374498	-34.837031	0.160154
-120.511381	-20.066886	0.165158
-124.073293	-35.948547	0.170163
-127.933737	-34.843649	0.175168
-132.134414	-36.940727	0.180173
-135.233948	-43.915769	0.185178
-139.447241	-37.579214	0.190182
-143.658445	-37.881673	0.195187
-147.234795	-27.245645	0.200192
-151.292850	-27.403802	0.205197
-154.393709	-24.321230	0.210202
-158.289180	-25.195995	0.215206
-162.013620	-31.170888	0.220211
-165.865720	-23.832252	0.225216
-169.812060	-25.594552	0.230221
-172.947144	-28.848733	0.235226
-176.682089	-23.173468	0.240230
-180.377942	-20.161488	0.245235
-184.268098	-31.586427	0.250240
-188.584173	-22.831785	0.255245
-191.992476	-22.174238	0.260250
-195.685251	-32.974671	0.265254
-199.779081	-29.351972	0.270259
-203.279607	-30.732797	0.275264
-207.194691	-22.961441	0.280269
-210.668546	-26.445346	0.285274
-214.773071	-29.194687	0.290278
-218.590693	-27.595029	0.295283
-221.972580	-24.089070	0.300288
-226.016942	-23.068199	0.305293
-229.543194	-23.618591	0.310298
-233.070834	-30.503105	0.315302
-236.797887	-14.554021	0.320307
-241.356850	-27.344933	0.325312
-245.394644	-23.101925	0.330317
-248.603380	-33.321964	0.335322
-252.161576	-13.954317	0.340326
-255.763738	-22.187759	0.345331
-259.324859	-26.275803	0.350336
-263.853185	-19.335262	0.355341
-267.674783	-29.126310	0.360346
-271.164020	-17.871681	0.365350
-274.660223	-29.004547	0.370355
-278.462744	-24.330704	0.375360
-282.135737	-23.376902	0.380365
-285.879020	-26.033977	0.385370
-290.164241	-17.250971	0.390374
-294.045225	-21.641127	0.395379
-297.395790	-22.178465	0.400384
-301.018502	-24.313892	0.405389
-304.447868	-21.560299	0.410394
-308.643217	-25.513911	0.415398
-312.220033	-14.637889	0.420403
-315.665425	-22.675496	0.425408
-320.266441	-15.299066	0.430413
-323.977685	-20.730207	0.435418
-327.627934	-16.757079	0.440422
-331.147443	-25.776266	0.445427
-334.411218	-21.631447	0.450432
-339.094862	-21.542766	0.455437
-342.563437	-32.553782	0.460442
-346.378789	-16.432765	0.465446
-350.107433	-24.975431	0.470451
-353.514672	-24.382478	0.475456
-357.608374	-14.614419	0.480461
-361.361836	-29.143683	0.485466
-365.261066	-19.783539	0.490470
-368.868725	-30.818039	0.495475
-372.596320	-25.269807	0.500480
-376.727064	-19.677699	0.505485
-379.878223	-25.254940	0.510490
-383.982633	-21.256523	0.515494
-387.930184	-27.015665	0.520499
-391.481743	-25.373065	0.525504
-395.665379	-24.416401	0.530509
-398.890304	-28.919017	0.535514
-402.363878	-29.909631	0.540518
-406.238464	-33.975780	0.545523
-409.907112	-30.420622	0.550528
-414.293473	-28.619462	0.555533
-417.920101	-29.631344	0.560538
-421.605939	-32.571752	0.565542
-425.376471	-35.534898	0.570547
-428.887812	-34.515226	0.575552
-433.185448	-22.976764	0.580557
-436.565713	-26.877383	0.585562
-440.587550	-30.218250	0.590566
-444.158131	-30.589366	0.595571
-447.796066	-37.665656	0.600576
-451.494280	-26.670722	0.605581
-455.187763	-27.578834	0.610586
-458.951469	-33.271021	0.615590
-462.809563	-26.702072	0.620595
-466.581937	-31.156588	0.625600
-470.844559	-21.823402	0.630605
-474.487596	-35.925418	0.635610
-478.148485	-35.055248	0.640614
-481.814437	-21.461990	0.645619
-485.019028	-36.365682	0.650624
-489.075080	-29.599506	0.655629
-492.923596	-28.830229	0.660634
-496.923800	-32.910856	0.665638
-500.729615	-32.878481	0.670643
-504.427448	-37.277033	0.675648
-508.140733	-24.215474	0.680653
-511.668478	-41.385522	0.685658
-515.329210	-34.250380	0.690662
-519.376357	-23.625373	0.695667
-523.222444	-31.270667	0.700672
-527.043935	-31.983188	0.705677
-530.866598	-35.637971	0.710682
-534.325807	-30.966535	0.715686
-538.106211	-27.396488	0.720691
-541.612203	-34.695545	0.725696
-545.843456	-25.092868	0.730701
-549.186447	-36.943592	0.735706
-553.235101	-38.308880	0.740710
-557.172670	-32.952327	0.745715
-560.765678	-26.206384	0.750720
-564.484559	-35.202812	0.755725
-568.207486	-33.013785	0.760730
-572.269780	-27.466979	0.765734
-575.936975	-38.474278	0.770739
-579.535990	-31.605931	0.775744
-583.386364	-16.563877	0.780749
-586.954458	-36.669816	0.785754
-590.702469	-23.596285	0.790758
-594.383396	-30.105683	0.795763
-598.068670	-28.644835	0.800768
-602.336671	-26.531096	0.805773
-606.029167	-32.111421	0.810778
-609.736436	-32.257034	0.815782
-613.745344	-18.827987	0.820787
-617.005394	-32.662960	0.825792
-621.124844	-32.258603	0.830797
-624.552430	-36.361109	0.835802
-628.179923	-25.812438	0.840806
-632.057321	-37.252817	0.845811
-635.874578	-32.110892	0.850816
-640.061211	-21.848166	0.855821
-643.356368	-36.448579	0.860826
-647.238342	-23.148569	0.865830
-651.065587	-31.504673	0.870835
-654.351328	-33.061066	0.875840
-658.597287	-24.837195	0.880845
-662.374073	-35.831572	0.885850
-665.817723	-27.346394	0.890854
-669.873423	-38.073852	0.895859
-673.469163	-37.037182	0.900864
-677.583786	-22.854747	0.905869
-681.131388	-32.130650	0.910874
-685.077415	-32.406720	0.915878
-688.627029	-30.987910	0.920883
-692.021245	-43.809462	0.925888
-695.941739	-33.406261	0.930893
-699.835405	-32.936926	0.935898
-703.834591	-36.050731	0.940902
-707.724089	-29.317120	0.945907
-711.292104	-34.474064	0.950912
-715.066901	-38.776403	0.955917
-718.841796	-29.326786	0.960922
-722.630293	-23.520724	0.965926
-726.463902	-26.115354	0.970931
-729.598370	-31.699504	0.975936
-734.037444	-28.640450	0.980941
-737.466223	-45.851159	0.985946
-741.357941	-32.972062	0.990950
-745.158087	-29.250312	0.995955
-748.701373	-28.770665	1.000960
-752.729915	-30.238168	1.005965
-755.994125	-39.675925	1.010970
-759.884542	-26.686622	1.015974
-763.943556	-32.712713	1.020979
-767.582818	-41.034005	1.025984
-771.764488	-29.280135	1.030989
-775.008317	-24.914004	1.035994
-778.651853	-23.836422	1.040998
-782.634576	-32.258910	1.046003
-786.206401	-39.425639	1.051008
-790.284281	-29.009749	1.056013
-794.011260	-50.939588	1.061018
-797.680817	-34.011816	1.066022
-801.504337	-31.364824	1.071027
-805.163264	-31.435860	1.076032
-809.060361	-30.443852	1.081037
-812.567457	-39.379101	1.086042
-816.749732	-23.238193	1.091046
-820.753721	-33.000710	1.096051
-824.017485	-31.908074	1.101056
-827.905362	-30.584788	1.106061
-831.478997	-40.387689	1.111066
-835.156015	-22.711223	1.116070
-838.986362	-31.180044	1.121075
-842.845926	-43.999506	1.126080
-846.953508	-44.366167	1.131085
-850.411134	-33.951569	1.136090
-853.862375	-41.607374	1.141094
-857.682445	-31.852301	1.146099
-861.432702	-32.561474	1.151104
-865.697218	-28.407348	1.156109
-869.642474	-40.648545	1.161114
-872.953547	-37.914639	1.166118
-876.817038	-34.668233	1.171123
-880.144293	-38.838432	1.176128
-884.055253	-37.722665	1.181133
-887.657454	-43.290156	1.186138
-891.787601	-32.862594	1.191142
-895.662545	-46.748619	1.196147
-899.270960	-39.957154	1.201152
-903.160679	-28.669193	1.206157
-906.475395	-43.466323	1.211162
-910.470781	-35.116518	1.216166
-914.462397	-31.065860	1.221171
-918.150268	-40.836163	1.226176
-922.354400	-37.487914	1.231181
-925.602491	-42.746128	1.236186
-929.568393	-37.920584	1.241190
-933.061832	-51.487512	1.246195
-936.758564	-34.812234	1.251200
-940.860175	-29.834090	1.256205
-944.230254	-45.779730	1.261210
-948.024007	-42.497056	1.266214
-951.963057	-37.062366	1.271219
-955.270383	-46.477158	1.276224
-959.280268	-35.748612	1.281229
-963.127947	-31.724044	1.286234
-967.047969	-39.779351	1.291238
-970.967145	-34.306808	1.296243
-974.457090	-34.357295	1.301248
-978.633799	-35.584681	1.306253
-981.885987	-37.303663	1.311258
-985.592096	-27.401045	1.316262
-989.721793	-40.810950	1.321267
-993.212689	-34.974800	1.326272
-997.285730	-35.157497	1.331277
-1000.828996	-42.248028	1.336282
-1004.724246	-39.751658	1.341286
-1008.387816	-33.585111	1.346291
-1012.202499	-43.163094	1.351296
-1015.884121	-28.804961	1.356301
-1019.341619	-39.578559	1.361306
-1023.395928	-37.619663	1.366310
-1027.326287	-39.334191	1.371315
-1030.876714	-33.067441	1.376320
-1034.870697	-35.467181	1.381325
-1038.596513	-42.053817	1.386330
-1042.278433	-33.377062	1.391334
-1046.060667	-29.657703	1.396339
-1049.673720	-42.178773	1.401344
-1053.471020	-23.817331	1.406349
-1057.061096	-42.818271	1.411354
-1061.232734	-40.247641	1.416358
-1064.857347	-35.804452	1.421363
-1068.299712	-34.574107	1.426368
-1072.155343	-36.565426	1.431373
-1076.005908	-38.748350	1.436378
-1079.751660	-38.838182	1.441382
-1083.799690	-37.337479	1.446387
-1087.451333	-40.867311	1.451392
-1091.476581	-29.678801	1.456397
-1094.957444	-26.225180	1.461402
-1098.666958	-36.532585	1.466406
-1102.041444	-35.696228	1.471411
-1105.978117	-42.354671	1.476416
-1110.171191	-37.695906	1.481421
-1113.644012	-37.116600	1.486426
-1117.504921	-28.988232	1.491430
-1121.368014	-33.193776	1.496435
-1124.706414	-42.284815	1.501440
-1128.607474	-32.442260	1.506445
-1132.286536	-38.687733	1.511450
-1136.208982	-32.593113	1.516454
-1140.105058	-41.926052	1.521459
-1143.501827	-42.136265	1.526464
-1147.526641	-36.170323	1.531469
-1151.193512	-43.001153	1.536474
-1154.930562	-41.901722	1.541478
-1158.582257	-32.458542	1.546483
-1162.498290	-40.911510	1.551488
-1166.566665	-36.151178	1.556493
-1170.331368	-36.255178	1.561498
-1173.933728	-36.394607	1.566502
-1177.572306	-43.548448	1.571507
-1181.114708	-41.754760	1.576512
-1185.418894	-38.882020	1.581517
-1188.651136	-46.846714	1.586522
-1192.767407	-32.693163	1.591526
-1196.676946	-35.971832	1.596531
-1200.257149	-36.898469	1.601536
-1204.090317	-36.329175	1.606541
-1207.611005	-35.882411	1.611546
-1211.402450	-38.587049	1.616550
-1215.135116	-34.091652	1.621555
-1218.940159	-45.033228	1.626560
-1222.909362	-36.929945	1.631565
-1226.446110	-44.177266	1.636570
-1230.416593	-41.066124	1.641574
-1234.024372	-38.869254	1.646579
-1237.482688	-46.515439	1.651584
-1241.716003	-27.680283	1.656589
-1245.330081	-38.543573	1.661594
-1249.351862	-40.692498	1.666598
-1252.883091	-49.077577	1.671603
-1256.458013	-44.607362	1.676608
-1260.437964	-37.853672	1.681613
-1263.805447	-36.114658	1.686618
-1267.900242	-34.929410	1.691622
-1272.047713	-25.450868	1.696627
-1275.487124	-33.388593	1.701632
-1279.144271	-37.065461	1.706637
-1282.526403	-41.535349	1.711642
-1286.561917	-29.554872	1.716646
-1290.520076	-30.045585	1.721651
-1294.106837	-42.456913	1.726656
-1298.120650	-16.598735	1.731661
-1301.862177	-28.755070	1.736666
-1305.242749	-39.508983	1.741670
-1309.397918	-38.350266	1.746675
-1313.091604	-44.694015	1.751680
-1317.061689	-34.335521	1.756685
-1320.817337	-35.162929	1.761690
-1324.215906	-37.302671	1.766694
-1327.909907	-36.422730	1.771699
-1331.741029	-39.046703	1.776704
-1335.596992	-34.228624	1.781709
-1339.185153	-38.886209	1.786714
-1343.160863	-35.745656	1.791718
-1346.995685	-28.401650	1.796723
-1350.387608	-41.949454	1.801728
-1354.466981	-34.272996	1.806733
-1358.113008	-39.108934	1.811738
-1361.817236	-49.137619	1.816742
-1365.860577	-33.528980	1.821747
-1369.445462	-36.958664	1.826752
-1373.429363	-33.293230	1.831757
-1376.503526	-43.752321	1.836762
-1380.478218	-45.192656	1.841766
-1384.516271	-36.672834	1.846771
-1388.023240	-43.164614	1.851776
-1392.241790	-36.484466	1.856781
-1395.935748	-41.085600	1.861786
-1399.775293	-35.030631	1.866790
-1403.473216	-40.567775	1.871795
-1406.607051	-40.840195	1.876800
-1410.723555	-36.021281	1.881805
-1414.724068	-36.736797	1.886810
-1418.249005	-47.484757	1.891814
-1422.135730	-34.458774	1.896819
-1425.914613	-38.942189	1.901824
-1430.007250	-31.668733	1.906829
-1433.092979	-46.742943	1.911834
-1436.899954	-43.361182	1.916838
-1440.969892	-39.574633	1.921843
-1444.494712	-40.859819	1.926848
-1448.496646	-38.971649	1.931853
-1452.194725	-35.981014	1.936858
-1455.892433	-39.453992	1.941862
-1460.108037	-37.358135	1.946867
-1463.217243	-47.270622	1.951872
-1467.259498	-42.840371	1.956877
-1470.929397	-37.996676	1.961882
-1474.633875	-40.066709	1.966886
-1478.657014	-32.476311	1.971891
-1482.000724	-39.533372	1.976896
-1486.144616	-42.791357	1.981901
-1489.710239	-39.752493	1.986906
-1493.616917	-40.405631	1.991910
-1497.758069	-32.659116	1.996915
-1501.752643	-39.417772	2.006912
-1501.901968	-37.217957	2.016909
-1499.713434	-39.159733	2.026906
-1496.909157	-35.980330	2.036902
-1494.684073	-34.842821	2.046899
-1492.792182	-37.924406	2.056896
-1490.875551	-37.133798	2.066893
-1488.890272	-35.809467	2.076890
-1487.417777	-35.176673	2.086886
-1485.214832	-35.473970	2.096883
-1483.426811	-40.143057	2.106880
-1481.498636	-37.178593	2.116877
-1479.402402	-38.469280	2.126874
-1477.994510	-34.567325	2.136870
-1476.017807	-32.087447	2.146867
-1473.716250	-30.793222	2.156864
-1471.707900	-32.407711	2.166861
-1470.128802	-28.916832	2.176858
-1468.132235	-29.604206	2.186854
-1466.287628	-32.128749	2.196851
-1464.411604	-31.168991	2.206848
-1462.600928	-40.537284	2.216845
-1460.598394	-33.064370	2.226842
-1458.892197	-29.895400	2.236838
-1456.896104	-36.880849	2.246835
-1454.874468	-30.254109	2.256832
-1452.895354	-38.155745	2.266829
-1451.039440	-36.802773	2.276826
-1449.492495	-34.028280	2.286822
-1447.653283	-34.033627	2.296819
-1445.498560	-36.767274	2.306816
-1443.761083	-40.561433	2.316813
-1442.251602	-38.016191	2.326810
-1439.557768	-36.912630	2.336806
-1437.876034	-36.351199	2.346803
-1436.371809	-34.242461	2.356800
-1434.443036	-42.006552	2.366797
-1432.395030	-29.793193	2.376794
-1430.389662	-40.457321	2.386790
-1428.778732	-40.625042	2.396787
-1426.459290	-41.992470	2.406784
-1424.850873	-35.845839	2.416781
-1423.235359	-27.044658	2.426778
-1421.115949	-30.337870	2.436774
-1419.373456	-31.485031	2.446771
-1417.030927	-37.168074	2.456768
-1415.349981	-39.811630	2.466765
-1413.844758	-40.012942	2.476762
-1411.927004	-40.275562	2.486758
-1409.826635	-32.661953	2.496755
-1407.860741	-32.813861	2.506752
-1405.970284	-30.485895	2.516749
-1404.229054	-37.907321	2.526746
-1402.211543	-39.524796	2.536742
-1400.570300	-33.992849	2.546739
-1398.569542	-34.458212	2.556736
-1396.674541	-38.798588	2.566733
-1394.707892	-32.480344	2.576730
-1392.790863	-38.489965	2.586726
-1391.340658	-38.822974	2.596723
-1389.405256	-39.756268	2.606720
-1387.306697	-37.330556	2.616717
-1385.342906	-47.130656	2.626714
-1383.513907	-35.076394	2.636710
-1381.645098	-34.650655	2.646707
-1379.410353	-38.911201	2.656704
-1378.034910	-43.703628	2.666701
-1376.078333	-35.053326	2.676698
-1373.986311	-36.974798	2.686694
-1372.204542	-38.241890	2.696691
-1370.431515	-37.170834	2.706688
-1368.376237	-39.225361	2.716685
-1366.698101	-34.174537	2.726682
-1364.853425	-39.370481	2.736678
-1363.075777	-31.762004	2.746675
-1360.773811	-35.187013	2.756672
-1359.166537	-36.955089	2.766669
-1357.414136	-42.057311	2.776666
-1355.246517	-38.831079	2.786662
-1353.532053	-41.110498	2.796659
-1351.459629	-40.737854	2.806656
-1349.975658	-37.972158	2.816653
-1347.692432	-43.047244	2.826650
-1346.064043	-29.104063	2.836646
-1343.998867	-40.676085	2.846643
-1342.263910	-42.137758	2.856640
-1340.505424	-34.199367	2.866637
-1338.464053	-39.977807	2.876634
-1336.547911	-39.673287	2.886630
-1334.551829	-39.997326	2.896627
-1332.906617	-35.463817	2.906624
-1331.042641	-42.372755	2.916621
-1328.889632	-36.992140	2.926618
-1327.088046	-36.882425	2.936614
-1325.243843	-29.518243	2.946611
-1323.502316	-36.885981	2.956608
-1321.683872	-39.080973	2.966605
-1319.585229	-36.255753	2.976602
-1317.841838	-34.159954	2.986598
-1316.065880	-39.998521	2.996595
-1313.949178	-31.536412	3.006592
-1311.929928	-39.640144	3.016589
-1310.679102	-38.231260	3.026586
-1308.485060	-37.290698	3.036582
-1306.701155	-36.713945	3.046579
-1304.701220	-38.495885	3.056576
-1302.577454	-35.573622	3.066573
-1300.877594	-34.091344	3.076570
-1299.377324	-36.844844	3.086566
-1297.070723	-33.329757	3.096563
-1295.172404	-30.606657	3.106560
-1293.568653	-44.001027	3.116557
-1291.608930	-39.301517	3.126554
-1289.663132	-36.582855	3.136550
-1287.740049	-48.083141	3.146547
-1285.694387	-38.356005	3.156544
-1284.143208	-33.984243	3.166541
-1282.129500	-42.694934	3.176538
-1280.144670	-44.116028	3.186534
-1278.370280	-40.675215	3.196531
-1276.430113	-40.063450	3.206528
-1274.454891	-38.961524	3.216525
-1272.986286	-39.510554	3.226522
-1271.058202	-39.938915	3.236518
-1269.040040	-41.687427	3.246515
-1267.133522	-39.780321	3.256512
-1264.899011	-39.337227	3.266509
-1263.766024	-40.048846	3.276506
-1261.419802	-43.214010	3.286502
-1259.489040	-38.906136	3.296499
-1257.748972	-40.232781	3.306496
-1255.863848	-44.604623	3.316493
-1254.130358	-38.321567	3.326490
-1252.128659	-45.145123	3.336486
-1249.912898	-46.320528	3.346483
-1248.363966	-48.822845	3.356480
-1246.688125	-48.782942	3.366477
-1244.701923	-45.336527	3.376474
-1242.779067	-48.137090	3.386470
-1240.867772	-40.680948	3.396467
-1239.209768	-45.117480	3.406464
-1236.918500	-41.025166	3.416461
-1235.352716	-46.897933	3.426458
-1233.303083	-41.873299	3.436454
-1231.586030	-45.520360	3.446451
-1229.622279	-40.567239	3.456448
-1227.670637	-44.010267	3.466445
-1225.885081	-39.303353	3.476442
-1224.004847	-36.752556	3.486438
-1221.874710	-41.386202	3.496435
-1220.160642	-35.399998	3.506432
-1218.532667	-40.196436	3.516429
-1216.657856	-37.785285	3.526426
-1214.641730	-37.544030	3.536422
-1212.691983	-41.413042	3.546419
-1210.884577	-42.692009	3.556416
-1208.851981	-35.599442	3.566413
-1206.879099	-43.935661	3.576410
-1205.168026	-36.752171	3.586406
-1203.464909	-33.310943	3.596403
-1201.551412	-41.669235	3.606400
-1199.331218	-39.670163	3.616397
-1197.438742	-46.533039	3.626394
-1195.828086	-35.599410	3.636390
-1194.232211	-41.216453	3.646387
-1192.334444	-43.798234	3.656384
-1190.125941	-44.542964	3.666381
-1188.366339	-44.761148	3.676378
-1186.225599	-42.611988	3.686374
-1184.576248	-40.145790	3.696371
-1182.709874	-40.010015	3.706368
-1180.831554	-39.659843	3.716365
-1178.987880	-41.590352	3.726362
-1176.896032	-45.516807	3.736358
-1175.144315	-29.851702	3.746355
-1173.097509	-38.528134	3.756352
-1171.514838	-48.063422	3.766349
-1169.636529	-47.441671	3.776346
-1167.682068	-48.857812	3.786342
-1165.903507	-43.210294	3.796339
-1164.026335	-48.046564	3.806336
-1161.915845	-44.507859	3.816333
-1159.991512	-46.389681	3.826330
-1158.193365	-37.353842	3.836326
-1156.489186	-41.856126	3.846323
-1154.705473	-38.898265	3.856320
-1152.462688	-49.148602	3.866317
-1150.731363	-43.488778	3.876314
-1149.146958	-49.129217	3.886310
-1146.803238	-42.792132	3.896307
-1145.036775	-46.387040	3.906304
-1143.589608	-47.474116	3.916301
-1141.326189	-50.910113	3.926298
-1139.524667	-52.672801	3.936294
-1137.780545	-41.758903	3.946291
-1135.739768	-44.030374	3.956288
-1133.573469	-40.240053	3.966285
-1132.157202	-44.271539	3.976282
-1130.201963	-44.757810	3.986278
-1127.938932	-39.926683	3.996275
-1126.214979	-37.205545	4.006272
-1124.596671	-44.995522	4.016269
-1122.721387	-48.468880	4.026266
-1120.866059	-41.161565	4.036262
-1119.077488	-46.010469	4.046259
-1117.169122	-39.761594	4.056256
-1115.142238	-42.411336	4.066253
-1112.707164	-41.886500	4.076250
-1111.540586	-40.203512	4.086246
-1109.590496	-43.369892	4.096243
-1107.615314	-39.408451	4.106240
-1105.814362	-43.226735	4.116237
-1103.695102	-36.855273	4.126234
-1101.989979	-39.224595	4.136230
-1100.125756	-43.708234	4.146227
-1098.268911	-35.752216	4.156224
-1096.417021	-39.749161	4.166221
-1094.317099	-37.967581	4.176218
-1092.849922	-34.351163	4.186214
-1090.840767	-32.701895	4.196211
-1088.747558	-38.892620	4.206208
-1086.925260	-35.631414	4.216205
-1084.968232	-43.851325	4.226202
-1083.269110	-37.960512	4.236198
-1081.037757	-33.826873	4.246195
-1079.574646	-38.442119	4.256192
-1077.870872	-39.488100	4.266189
-1075.532022	-45.684946	4.276186
-1073.712076	-39.788191	4.286182
-1071.997102	-35.737730	4.296179
-1070.059155	-37.858492	4.306176
-1068.056535	-45.261503	4.316173
-1066.467847	-36.299443	4.326170
-1064.494603	-35.684896	4.336166
-1062.506118	-42.263042	4.346163
-1060.957304	-44.717855	4.356160
-1058.957313	-43.040254	4.366157
-1056.625829	-42.419845	4.376154
-1055.187947	-43.739059	4.386150
-1053.072511	-38.806882	4.396147
-1051.146205	-43.576720	4.406144
-1049.497470	-46.004877	4.416141
-1047.635673	-43.190468	4.426138
-1045.612792	-45.384792	4.436134
-1043.818860	-46.970938	4.446131
-1042.142650	-32.346753	4.456128
-1040.302026	-36.310278	4.466125
-1038.221510	-39.063268	4.476122
-1036.200520	-45.479229	4.486118
-1034.437704	-44.840474	4.496115
-1032.388111	-43.279727	4.506112
-1030.687816	-42.960958	4.516109
-1028.714018	-45.990543	4.526106
-1027.040584	-52.463009	4.536102
-1024.923088	-42.612901	4.546099
-1023.243765	-45.735907	4.556096
-1021.317446	-46.173253	4.566093
-1019.184857	-49.285066	4.576090
-1017.495365	-46.964109	4.586086
-1016.030936	-43.915602	4.596083
-1014.072810	-52.124580	4.606080
-1011.982276	-38.902376	4.616077
-1010.036361	-43.152706	4.626074
-1007.969762	-42.355680	4.636070
-1006.070232	-42.103492	4.646067
-1004.409979	-36.687961	4.656064
-1002.747579	-44.251241	4.666061
-1000.600073	-45.090246	4.676058
-998.745591	-47.169181	4.686054
-997.109890	-49.544694	4.696051
-995.153014	-49.312720	4.706048
-993.074649	-48.893338	4.716045
-991.221709	-46.028521	4.726042
-989.478818	-47.181743	4.736038
-987.573029	-51.108279	4.746035
-985.844219	-39.391302	4.756032
-983.831873	-46.075829	4.766029
-981.510873	-48.193041	4.776026
-979.934410	-48.321783	4.786022
-978.183341	-38.447764	4.796019
-976.429627	-44.745150	4.806016
-974.391610	-36.409062	4.816013
-972.339571	-44.388303	4.826010
-970.501447	-40.573765	4.836006
-968.884637	-43.055182	4.846003
-966.724429	-41.516800	4.856000
-965.119093	-43.622183	4.865997
-963.426713	-38.472275	4.875994
-961.319053	-42.593700	4.885990
-959.356372	-38.109095	4.895987
-957.538961	-41.674122	4.905984
-955.395502	-42.531386	4.915981
-953.677103	-46.094787	4.925978
-951.718583	-44.888865	4.935974
-950.002737	-43.288886	4.945971
-948.358831	-36.388121	4.955968
-946.466711	-49.171592	4.965965
-944.200189	-37.267410	4.975962
-942.302053	-45.645160	4.985958
-940.575285	-45.753701	4.995955
-939.225569	-38.406429	5.005952
-937.023064	-40.376762	5.015949
-934.920992	-37.802775	5.025946
-933.190488	-42.197017	5.035942
-931.272714	-38.579911	5.045939
-929.285444	-37.684871	5.055936
-927.283104	-40.044753	5.065933
-925.538916	-32.056357	5.075930
-923.707858	-34.807257	5.085926
-921.764841	-41.142770	5.095923
-920.151125	-40.427985	5.105920
-918.232368	-36.777869	5.115917
-916.300352	-34.861913	5.125914
-914.177439	-40.146223	5.135910
-912.581448	-44.168428	5.145907
-910.736139	-37.707189	5.155904
-908.786066	-37.339849	5.165901
-906.716872	-39.172002	5.175898
-905.078781	-40.914700	5.185894
-903.015771	-33.286724	5.195891
-901.080058	-32.954974	5.205888
-899.330488	-33.790263	5.215885
-897.199683	-26.181010	5.225882
-895.695421	-36.185174	5.235878
-893.919907	-31.042186	5.245875
-891.583200	-25.142629	5.255872
-889.915133	-29.271082	5.265869
-887.970931	-28.065972	5.275866
-886.259862	-30.120316	5.285862
-884.471521	-23.452579	5.295859
-882.566315	-22.866471	5.305856
-880.803516	-29.924699	5.315853
-878.365433	-27.061758	5.325850
-876.564520	-41.714227	5.335846
-875.148057	-28.219902	5.345843
-873.254932	-32.318009	5.355840
-871.021383	-23.403622	5.365837
-869.148980	-28.982573	5.375834
-867.657967	-28.177085	5.385830
-865.695646	-35.587712	5.395827
-863.559047	-31.009249	5.405824
-861.861683	-28.896266	5.415821
-860.064782	-32.229006	5.425818
-857.802778	-34.320879	5.435814
-855.919570	-30.327141	5.445811
-854.466110	-28.568306	5.455808
-852.540012	-23.531456	5.465805
-850.608466	-27.926205	5.475802
-848.460889	-28.600879	5.485798
-846.821048	-24.520861	5.495795
-844.917869	-23.667566	5.505792
-843.003135	-26.842295	5.515789
-841.214792	-35.125061	5.525786
-839.186458	-33.222859	5.535782
-837.379738	-30.180003	5.545779
-835.864780	-30.884586	5.555776
-833.876078	-32.321718	5.565773
-831.750325	-33.703390	5.575770
-829.684062	-31.625669	5.585766
-828.079511	-32.341411	5.595763
-826.231439	-25.746330	5.605760
-824.116052	-25.886907	5.615757
-822.613803	-27.862039	5.625754
-820.545339	-26.449375	5.635750
-818.756514	-22.765769	5.645747
-816.779894	-29.922867	5.655744
-814.409886	-24.666424	5.665741
-813.082567	-27.756708	5.675738
-811.449072	-23.140404	5.685734
-809.295209	-26.222282	5.695731
-807.209216	-31.489550	5.705728
-805.627748	-22.458233	5.715725
-803.679983	-28.349172	5.725722
-801.587216	-24.191521	5.735718
-800.152681	-23.356436	5.745715
-798.078517	-20.247351	5.755712
-796.072254	-22.955111	5.765709
-793.980515	-28.046452	5.775706
-792.398091	-21.432563	5.785702
-790.605020	-26.023021	5.795699
-788.794248	-28.067971	5.805696
-786.886005	-29.896400	5.815693
-784.799090	-27.447741	5.825690
-783.085187	-30.459276	5.835686
-781.165121	-25.631393	5.845683
-779.206547	-20.446515	5.855680
-777.351938	-33.670721	5.865677
-775.426472	-33.226707	5.875674
-773.570917	-30.692115	5.885670
-771.887185	-34.199329	5.895667
-769.954746	-27.085597	5.905664
-767.628790	-24.637233	5.915661
-766.127823	-30.988821	5.925658
-764.379323	-32.261194	5.935654
-762.381683	-30.873474	5.945651
-760.525031	-29.711105	5.955648
-758.344458	-35.283964	5.965645
-756.898992	-35.601614	5.975642
-754.839137	-30.518166	5.985638
-753.235219	-34.950474	5.995635
-750.952173	-37.917160	6.005632
-749.309658	-27.414556	6.015629
-747.174604	-30.959147	6.025626
-745.296799	-22.391970	6.035622
-743.805182	-27.624195	6.045619
-741.826152	-20.773661	6.055616
-739.949196	-25.470645	6.065613
-737.886929	-18.732879	6.075610
-735.941547	-26.773844	6.085606
-734.162270	-27.593233	6.095603
-732.314970	-20.192709	6.105600
-730.823415	-27.545374	6.115597
-728.712475	-22.200071	6.125594
-726.538390	-25.675096	6.135590
-725.019120	-28.458125	6.145587
-722.794162	-29.448199	6.155584
-721.009206	-31.258454	6.165581
-719.157955	-24.662209	6.175578
-717.361641	-26.486908	6.185574
-715.454833	-23.291005	6.195571
-713.664921	-28.785611	6.205568
-711.559724	-32.645915	6.215565
-710.027567	-22.894562	6.225562
-707.985458	-25.227464	6.235558
-705.771541	-26.155761	6.245555
-704.493393	-25.169315	6.255552
-702.404834	-18.265196	6.265549
-700.356102	-28.001017	6.275546
-698.729442	-29.165454	6.285542
-696.411758	-23.210547	6.295539
-694.644337	-33.352972	6.305536
-693.026919	-26.517242	6.315533
-691.258665	-24.399670	6.325530
-689.067866	-27.769967	6.335526
-687.348269	-27.668763	6.345523
-685.202197	-27.984639	6.355520
-683.694908	-28.989470	6.365517
-681.613436	-32.842800	6.375514
-679.620282	-26.354458	6.385510
-678.155800	-28.443463	6.395507
-676.240418	-21.446914	6.405504
-674.341204	-26.602128	6.415501
-672.224612	-30.843155	6.425498
-670.354554	-30.871765	6.435494
-668.471348	-28.763071	6.445491
-666.552674	-33.872439	6.455488
-664.766832	-28.489343	6.465485
-663.053896	-31.252753	6.475482
-660.827827	-34.729709	6.485478
-659.196027	-23.344292	6.495475
-657.380013	-19.484907	6.505472
-655.348407	-25.419130	6.515469
-653.373593	-27.215462	6.525466
-651.708965	-37.289329	6.535462
-649.870686	-25.409546	6.545459
-648.025495	-28.855635	6.555456
-646.044271	-34.074453	6.565453
-644.054762	-37.120451	6.575450
-642.247532	-33.081239	6.585446
-640.426313	-35.517734	6.595443
-638.590302	-37.081882	6.605440
-636.652919	-27.036810	6.615437
-634.624619	-34.803585	6.625434
-632.719050	-36.415157	6.635430
-631.174186	-35.907060	6.645427
-629.218113	-33.211574	6.655424
-627.025037	-29.851342	6.665421
-625.331220	-29.794919	6.675418
-623.497979	-26.833495	6.685414
-621.873011	-27.617096	6.695411
-619.726084	-27.557273	6.705408
-617.846714	-31.962453	6.715405
-615.750696	-31.753971	6.725402
-614.180650	-34.827666	6.735398
-612.584810	-29.231021	6.745395
-610.342756	-31.120536	6.755392
-608.558790	-29.041726	6.765389
-606.628851	-30.276657	6.775386
-604.773008	-33.006017	6.785382
-602.892376	-27.975898	6.795379
-601.061298	-32.261249	6.805376
-599.016511	-36.006021	6.815373
-597.476220	-34.069848	6.825370
-595.535984	-29.848167	6.835366
-593.173705	-38.432449	6.845363
-591.725763	-26.196582	6.855360
-589.720803	-33.012256	6.865357
-588.078226	-28.004093	6.875354
-586.132587	-31.750384	6.885350
-583.775964	-30.279335	6.895347
-582.018932	-27.218864	6.905344
-580.431170	-36.925159	6.915341
-578.372739	-31.467122	6.925338
-576.666177	-32.607926	6.935334
-574.775585	-27.352013	6.945331
-573.097455	-30.630837	6.955328
-571.298985	-26.482801	6.965325
-569.196011	-30.759459	6.975322
-566.897551	-33.720543	6.985318
-565.299106	-31.173131	6.995315
-563.529922	-31.450798	7.005312
-561.472037	-29.649385	7.015309
-559.676341	-30.842309	7.025306
-557.724134	-32.868628	7.035302
-556.014641	-30.687884	7.045299
-554.009641	-33.044728	7.055296
-552.349528	-31.872904	7.065293
-550.467485	-27.809252	7.075290
-548.351124	-23.693027	7.085286
-546.548230	-29.391689	7.095283
-544.773128	-27.224575	7.105280
-543.057859	-28.635159	7.115277
-540.859325	-27.628274	7.125274
-538.956727	-31.189238	7.135270
-537.252592	-31.529125	7.145267
-535.353159	-24.092552	7.155264
-533.564471	-23.907537	7.165261
-531.569512	-23.985987	7.175258
-529.433915	-30.175134	7.185254
-527.973751	-30.458678	7.195251
-526.007247	-28.925260	7.205248
-523.961085	-31.711799	7.215245
-522.019894	-28.467545	7.225242
-520.312673	-28.244247	7.235238
-518.773263	-34.557626	7.245235
-516.750592	-27.293874	7.255232
-514.560166	-31.685504	7.265229
-512.992607	-32.783536	7.275226
-510.890574	-34.184820	7.285222
-509.082648	-32.015027	7.295219
-507.189324	-31.832495	7.305216
-505.416896	-27.234997	7.315213
-503.172730	-25.804326	7.325210
-501.713468	-26.717691	7.335206
-499.571142	-34.999927	7.345203
-497.890187	-26.371095	7.355200
-495.783507	-31.988770	7.365197
-494.013744	-32.912248	7.375194
-492.190606	-28.933874	7.385190
-490.600644	-35.391095	7.395187
-488.236262	-34.435911	7.405184
-486.494247	-27.455720	7.415181
-484.647780	-28.040926	7.425178
-482.889221	-30.129414	7.435174
-480.821959	-24.645853	7.445171
-478.925707	-30.717788	7.455168
-477.274977	-28.554442	7.465165
-475.003783	-31.803182	7.475162
-473.381816	-26.407969	7.485158
-471.627278	-25.846413	7.495155
-469.636388	-29.325112	7.505152
-467.633362	-31.544206	7.515149
-465.956069	-31.431349	7.525146
-464.340750	-36.615274	7.535142
-461.931003	-33.831049	7.545139
-460.330767	-32.011723	7.555136
-458.449586	-31.942472	7.565133
-456.449025	-30.163390	7.575130
-454.392952	-32.809353	7.585126
-452.999530	-29.914920	7.595123
-450.703142	-22.904809	7.605120
-448.976562	-28.521746	7.615117
-447.407993	-29.937257	7.625114
-445.217856	-34.551405	7.635110
-443.402623	-32.246941	7.645107
-441.394244	-32.155359	7.655104
-439.917732	-27.508977	7.665101
-437.806516	-32.434191	7.675098
-435.760940	-28.527605	7.685094
-434.124881	-35.153202	7.695091
-431.979264	-25.886433	7.705088
-430.215466	-26.243666	7.715085
-428.333332	-33.077497	7.725082
-426.526681	-28.438035	7.735078
-424.550105	-37.356881	7.745075
-422.719247	-37.451667	7.755072
-420.891767	-27.486738	7.765069
-419.043991	-34.754010	7.775066
-417.144961	-35.077566	7.785062
-415.115507	-33.206749	7.795059
-413.249211	-27.965765	7.805056
-411.843868	-28.976254	7.815053
-409.565936	-32.104434	7.825050
-407.616847	-38.203698	7.835046
-405.648997	-34.687296	7.845043
-404.156289	-38.024818	7.855040
-402.150771	-38.799563	7.865037
-400.238166	-28.671372	7.875034
-398.261448	-28.615750	7.885030
-396.573933	-32.813297	7.895027
-394.331742	-31.634830	7.905024
-392.965217	-32.354908	7.915021
-390.809695	-33.374640	7.925018
-389.120862	-34.518797	7.935014
-386.961693	-33.611270	7.945011
-385.204918	-34.652592	7.955008
-383.416452	-27.283430	7.965005
-381.558063	-30.204077	7.975002
-379.684734	-29.977200	7.984998
-377.729936	-33.007970	7.994995
-375.863546	-30.765305	8.004992
-373.694589	-35.770734	8.014989
-372.104178	-34.565550	8.024986
-370.175910	-27.875520	8.034982
-368.424160	-30.763343	8.044979
-366.488730	-26.258073	8.054976
-364.786939	-28.162156	8.064973
-362.387273	-31.797610	8.074970
-360.872074	-34.123464	8.084966
-359.008213	-32.582992	8.094963
-357.111137	-27.378454	8.104960
-355.195876	-25.162519	8.114957
-353.232329	-28.627288	8.124954
-351.685272	-25.109970	8.134950
-349.494761	-25.372643	8.144947
-347.425961	-26.323230	8.154944
-346.052876	-30.097925	8.164941
-344.008760	-29.126203	8.174938
-341.979858	-28.350991	8.184934
-340.006507	-31.649950	8.194931
-338.222890	-25.792563	8.204928
-336.273667	-20.653170	8.214925
-334.475742	-22.907307	8.224922
-332.587032	-27.779546	8.234918
-331.105570	-33.646211	8.244915
-329.332275	-20.546322	8.254912
-326.958904	-27.491662	8.264909
-325.297462	-22.659993	8.274906
-323.313693	-24.189074	8.284902
-321.211023	-31.670651	8.294899
-319.458599	-24.761456	8.304896
-317.838053	-21.596889	8.314893
-315.839744	-27.811312	8.324890
-313.742716	-27.787457	8.334886
-312.010570	-19.436636	8.344883
-310.165506	-23.916640	8.354880
-308.353402	-23.798351	8.364877
-306.339874	-24.639031	8.374874
-304.956099	-26.778088	8.384870
-302.783761	-33.877624	8.394867
-300.690399	-30.431691	8.404864
-298.817251	-34.284605	8.414861
-297.012579	-31.252046	8.424858
-295.155273	-30.649924	8.434854
-293.226744	-27.515557	8.444851
-291.334945	-25.117409	8.454848
-289.390531	-30.017454	8.464845
-287.700380	-27.468698	8.474842
-285.776916	-25.080337	8.484838
-283.811997	-32.707259	8.494835
-282.089408	-32.577819	8.504832
-280.264480	-29.210595	8.514829
-278.417577	-27.203154	8.524826
-276.439290	-29.152889	8.534822
-274.249732	-33.400492	8.544819
-272.631224	-33.649158	8.554816
-270.866806	-27.963912	8.564813
-268.880444	-24.794545	8.574810
-266.970923	-27.849582	8.584807
-265.097018	-30.884721	8.594803
-263.232796	-31.477329	8.604800
-261.549657	-26.375927	8.614797
-259.437423	-30.879589	8.624794
-257.475375	-39.687050	8.634791
-255.721642	-33.450630	8.644787
-253.869342	-32.955042	8.654784
-252.008001	-30.165170	8.664781
-250.373141	-32.680579	8.674778
-248.426895	-32.064196	8.684775
-246.260731	-28.374050	8.694771
-244.512328	-29.784977	8.704768
-242.475445	-21.556948	8.714765
-240.539630	-28.272904	8.724762
-239.020098	-26.413703	8.734759
-237.210552	-24.592893	8.744755
-235.162456	-25.816389	8.754752
-233.086871	-28.140030	8.764749
-231.130417	-31.551467	8.774746
-229.587608	-34.110590	8.784743
-227.460572	-33.251473	8.794739
-225.637295	-33.581734	8.804736
-223.780681	-42.653387	8.814733
-221.943510	-41.863263	8.824730
-220.078107	-43.305476	8.834727
-218.125154	-36.205584	8.844723
-216.234836	-42.173749	8.854720
-214.639244	-37.290442	8.864717
-212.725497	-38.175118	8.874714
-210.733028	-41.680703	8.884711
-208.807396	-42.071496	8.894707
-206.779671	-38.757107	8.904704
-205.120136	-43.425310	8.914701
-203.152777	-41.853866	8.924698
-201.430143	-36.485574	8.934695
-199.260635	-35.443741	8.944691
-197.626132	-38.868507	8.954688
-196.018275	-41.172733	8.964685
-193.945686	-38.009172	8.974682
-192.027882	-47.033725	8.984679
-189.972705	-41.945857	8.994675
-188.378363	-46.955740	9.004672
-186.527872	-42.263088	9.014669
-184.248767	-38.701434	9.024666
-182.560520	-39.782199	9.034663
-180.608007	-40.982501	9.044659
-179.061275	-44.893759	9.054656
-176.958261	-40.762433	9.064653
-174.798241	-39.460125	9.074650
-173.027442	-42.650841	9.084647
-171.527644	-44.074147	9.094643
-169.492421	-42.641396	9.104640
-167.879113	-41.627618	9.114637
-165.672596	-40.555346	9.124634
-163.733882	-41.338181	9.134631
-162.035956	-45.630388	9.144627
-160.143108	-45.602238	9.154624
-158.311325	-42.652845	9.164621
-156.329083	-44.137337	9.174618
-154.194063	-40.050571	9.184615
-152.351757	-38.181242	9.194611
-150.844023	-38.986872	9.204608
-148.870356	-40.814191	9.214605
-147.080720	-40.081160	9.224602
-144.933694	-40.445653	9.234599
-143.139298	-48.072096	9.244595
-141.558535	-40.235400	9.254592
-139.285894	-45.336119	9.264589
-137.662658	-48.972198	9.274586
-135.833406	-40.478851	9.284583
-133.773451	-33.913837	9.294579
-131.819160	-37.926414	9.304576
-129.884514	-42.835829	9.314573
-128.347753	-38.097806	9.324570
-126.290392	-38.477974	9.334567
-124.099386	-31.261247	9.344563
-122.580888	-30.683877	9.354560
-120.960467	-29.737515	9.364557
-118.903754	-28.958657	9.374554
-117.024812	-31.479767	9.384551
-115.124472	-27.071313	9.394547
-113.217545	-26.459599	9.404544
-111.053773	-29.239303	9.414541
-109.276509	-22.485476	9.424538
-107.755662	-25.205229	9.434535
-105.597554	-25.408827	9.444531
-103.660698	-23.249815	9.454528
-102.025900	-26.532468	9.464525
-100.202745	-30.154636	9.474522
-98.156276	-26.873138	9.484519
-96.224971	-29.650475	9.494515
-94.262086	-24.945674	9.504512
-92.435056	-21.990729	9.514509
-90.548881	-22.605654	9.524506
-88.821540	-29.477708	9.534503
-87.375058	-27.284657	9.544499
-84.925997	-27.949909	9.554496
-82.964338	-22.359135	9.564493
-81.344253	-23.845788	9.574490
-79.667292	-26.694638	9.584487
-77.470802	-24.139668	9.594483
-75.565632	-20.031942	9.604480
-73.701863	-20.736436	9.614477
-71.966843	-26.618151	9.624474
-69.807676	-28.757627	9.634471
-68.167076	-27.901288	9.644467
-66.239798	-22.676058	9.654464
-64.438397	-26.991030	9.664461
-62.432390	-24.225663	9.674458
-60.591427	-28.186951	9.684455
-58.938349	-30.084632	9.694451
-56.898745	-28.938264	9.704448
-55.171535	-30.023579	9.714445
-53.195158	-22.704645	9.724442
-51.034591	-30.182615	9.734439
-49.404986	-31.973916	9.744435
-47.679267	-26.962827	9.754432
-45.649168	-27.127005	9.764429
-43.549030	-22.745626	9.774426
-42.103619	-34.146769	9.784423
-39.781443	-24.413576	9.794419
-38.038893	-31.191710	9.804416
-36.533576	-22.646593	9.814413
-34.590943	-25.228328	9.824410
-32.441458	-30.201945	9.834407
-30.529464	-25.602653	9.844403
-28.827611	-25.847084	9.854400
-27.047009	-22.452060	9.864397
-24.927561	-24.749368	9.874394
-22.734120	-28.473179	9.884391
-20.980054	-31.459023	9.894387
-19.376448	-26.482116	9.904384
-17.849315	-27.308127	9.914381
-15.949186	-22.849031	9.924378
-13.587199	-24.783974	9.934375
-11.633223	-20.680823	9.944371
-9.908596	-29.240247	9.954368
-7.956652	-28.120906	9.964365
-6.499120	-17.954499	9.974362
-4.953451	0.081361	9.984359
-3.760512	31.302176	9.994355
-2.279856	86.418323	10.004352
-1.014879	145.000092	10.014349
0.000000	203.720208	10.019354
0.661969	256.474566	10.024359
1.336146	280.915070	10.029363
1.684433	337.436565	10.034368
2.049927	350.697116	10.039373
2.718242	386.486330	10.044378
2.781797	402.901651	10.049383
3.218407	417.702627	10.054387
2.996829	438.818590	10.059392
3.376284	445.666742	10.064397
3.335896	473.449547	10.069402
3.228209	475.494775	10.074407
4.015434	482.162788	10.079411
3.627233	501.553433	10.084416
3.859577	511.500129	10.089421
3.936186	513.050767	10.094426
3.930061	517.161373	10.099431
4.023391	516.706620	10.104435
4.340896	546.203391	10.109440
5.108589	540.725717	10.114445
4.615993	532.866020	10.119450
4.429183	545.506796	10.124455
4.870694	525.874404	10.129459
4.683470	536.685976	10.134464
4.814173	537.319665	10.139469
4.805800	537.469336	10.144474
4.644751	539.319659	10.149479
4.851688	542.330269	10.154483
4.428388	549.815869	10.159488
4.777339	553.772079	10.164493
4.864725	573.377121	10.169498
4.819564	580.146409	10.174503
5.133212	579.880441	10.179507
5.118236	586.350027	10.184512
5.367730	591.191013	10.189517
5.338594	585.960268	10.194522
5.250316	581.926405	10.199527
5.267337	591.489608	10.204531
4.931126	587.359672	10.209536
5.393714	592.281787	10.214541
5.174721	593.512152	10.219546
5.163437	600.528360	10.224551
5.395134	591.811934	10.229555
5.222090	605.694784	10.234560
5.098114	594.352682	10.239565
5.074969	614.426420	10.244570
5.599496	621.283056	10.249575
5.915231	635.048549	10.254579
5.678579	638.475288	10.259584
5.575508	634.751278	10.264589
5.439403	638.100478	10.269594
5.505747	635.557397	10.274599
5.821659	640.458770	10.279603
5.975454	651.540888	10.284608
6.059841	637.625030	10.289613
5.775035	645.244708	10.294618
5.966326	642.494039	10.299623
6.012216	648.838826	10.304627
5.893963	643.559196	10.309632
6.407416	659.830508	10.314637
6.195821	664.585791	10.319642
6.121062	685.502073	10.324647
6.487666	679.910126	10.329651
6.331136	692.101494	10.334656
6.229711	687.110903	10.339661
6.367738	702.437616	10.344666
6.461354	689.272451	10.349671
6.416307	689.729174	10.354675
6.218621	702.881181	10.359680
6.589355	704.539469	10.364685
6.699254	698.630487	10.369690
6.620372	702.462589	10.374695
6.957432	703.568001	10.379699
6.551359	709.502351	10.384704
6.823552	703.286781	10.389709
6.666618	709.949377	10.394714
6.767539	705.364903	10.399719
6.855461	714.334975	10.404723
6.816295	742.720502	10.409728
7.011917	734.637380	10.414733
6.915004	757.192620	10.419738
6.721973	751.010233	10.424743
7.194068	742.766312	10.429747
6.993519	757.797000	10.434752
7.256724	749.237883	10.439757
7.296173	750.606814	10.444762
7.120029	749.535861	10.449767
7.580265	742.071280	10.454771
7.373906	758.536364	10.459776
7.570975	747.034124	10.464781
7.545631	748.337694	10.469786
7.199402	765.515810	10.474791
7.719648	781.328853	10.479795
7.555784	787.439071	10.484800
7.591823	796.430085	10.489805
7.494141	789.450292	10.494810
7.521140	799.860454	10.499815
7.886973	797.897214	10.504819
7.622052	803.627736	10.509824
7.946373	798.252226	10.514829
7.831853	805.732861	10.519834
7.852145	804.200056	10.524839
8.411872	808.088024	10.529843
8.215407	810.789290	10.534848
7.890059	802.467523	10.539853
8.080061	822.550129	10.544858
8.237951	831.116445	10.549863
8.388216	829.132391	10.554867
8.162595	842.853539	10.559872
8.356122	844.087514	10.564877
8.134803	845.151111	10.569882
7.879908	836.915859	10.574887
8.368676	840.255325	10.579891
8.315361	843.414744	10.584896
8.367344	840.530136	10.589901
8.419653	860.481790	10.594906
8.651737	872.064110	10.599911
9.054427	868.294063	10.604915
8.727763	877.928042	10.609920
8.868372	875.838286	10.614925
8.809730	876.018057	10.619930
9.016437	874.476012	10.624935
8.990870	878.570897	10.629939
8.958449	883.228285	10.634944
8.947694	888.213386	10.639949
9.006243	885.204717	10.644954
8.452605	889.990975	10.649959
9.263057	884.848561	10.654963
9.092059	883.344682	10.659968
9.261220	888.343665	10.664973
8.996421	882.831850	10.669978
8.725345	889.287224	10.674983
9.135533	899.945429	10.679987
9.469128	914.908429	10.684992
9.428901	921.568276	10.689997
9.513117	920.194002	10.695002
9.632727	932.731043	10.700007
9.914901	917.542277	10.705011
9.752018	917.249806	10.710016
9.693766	926.661229	10.715021
9.866662	913.721341	10.720026
9.584240	927.541517	10.725031
9.798689	940.058707	10.730035
9.918124	935.669909	10.735040
9.735022	926.716661	10.740045
9.802233	932.687579	10.745050
9.615062	934.810205	10.750055
10.068645	931.298537	10.755059
10.183487	933.869745	10.760064
10.028799	940.808062	10.765069
10.316097	937.504270	10.770074
10.185579	936.064893	10.775079
10.241937	940.059994	10.780083
10.265805	951.530505	10.785088
10.508137	958.642055	10.790093
10.459087	973.759191	10.795098
10.581509	967.300885	10.800103
10.579447	957.886645	10.805107
10.365632	965.995074	10.810112
10.475400	963.973305	10.815117
10.489115	972.406578	10.820122
10.494795	981.962385	10.825127
10.762902	969.671178	10.830131
10.588301	978.535050	10.835136
10.845859	974.859090	10.840141
11.094411	970.091708	10.845146
10.739188	982.464825	10.850151
10.807897	970.202268	10.855155
10.649346	978.079533	10.860160
10.442011	976.370122	10.865165
11.016482	981.266642	10.870170
10.854499	999.256974	10.875175
11.315116	1001.058661	10.880179
11.214646	1016.718646	10.885184
11.372181	1006.181325	10.890189
11.610575	1005.753884	10.895194
11.388075	1001.230364	10.900199
11.514775	999.344666	10.905203
11.263567	1002.706000	10.910208
11.342610	1014.082601	10.915213
11.613691	1008.338603	10.920218
11.521811	1015.896162	10.925223
11.801386	1005.878710	10.930227
11.616310	1019.560441	10.935232
11.629343	1015.519760	10.940237
11.833733	1015.039393	10.945242
11.342815	1021.788519	10.950247
11.990020	1012.275416	10.955251
11.945368	1020.725913	10.960256
11.800968	1019.441711	10.965261
11.575841	1017.668899	10.970266
11.660778	1028.711824	10.975271
11.989601	1014.075353	10.980275
11.979282	1024.538939	10.985280
12.009483	1025.187104	10.990285
11.735365	1027.646897	10.995290
11.917184	1046.628794	11.000295
12.250465	1046.113674	11.005299
12.422258	1055.726615	11.010304
12.312983	1058.939163	11.015309
12.561409	1055.595812	11.020314
12.348920	1066.601047	11.025319
12.232394	1046.415121	11.030323
12.393746	1059.568532	11.035328
12.109740	1052.448014	11.040333
12.353790	1060.645897	11.045338
12.511268	1060.020042	11.050343
12.687927	1056.121991	11.055347
12.253943	1060.108600	11.060352
12.603043	1070.011825	11.065357
12.646191	1085.426619	11.070362
12.668692	1087.917963	11.075367
13.018896	1083.869217	11.080371
12.741081	1095.610319	11.085376
13.010180	1095.330948	11.090381
12.831444	1082.212022	11.095386
13.187491	1101.238742	11.100391
13.146109	1093.683675	11.105395
12.814977	1089.194802	11.110400
13.006637	1084.671431	11.115405
12.885381	1099.896413	11.120410
13.378176	1108.215504	11.125415
13.560356	1116.828580	11.130419
13.376015	1126.936782	11.135424
13.477638	1129.891771	11.140429
13.930703	1123.502089	11.145434
13.465050	1121.431723	11.150439
13.513987	1104.743951	11.155443
13.656201	1121.108114	11.160448
14.042637	1117.428910	11.165453
13.936527	1099.878015	11.170458
13.637572	1095.754605	11.175463
13.890871	1088.715532	11.180467
13.600320	1087.822078	11.185472
13.997691	1105.643686	11.190477
14.216071	1095.024053	11.195482
14.060741	1089.419002	11.200487
13.951931	1090.696490	11.205491
13.631136	1100.014277	11.210496
14.031251	1109.994553	11.215501
14.218808	1128.884175	11.220506
13.976988	1136.432594	11.225511
14.402944	1129.365962	11.230515
14.095205	1132.408323	11.235520
14.226947	1125.342887	11.240525
14.185754	1128.552476	11.245530
14.199365	1137.145140	11.250535
14.381328	1133.809218	11.255539
14.271769	1133.765291	11.260544
14.641471	1121.057191	11.265549
14.609123	1124.374182	11.270554
14.457599	1141.247284	11.275559
14.809117	1131.530521	11.280563
14.508910	1135.440616	11.285568
14.607468	1143.041986	11.290573
14.844934	1134.206040	11.295578
14.940852	1147.035640	11.300583
15.122193	1150.783774	11.305587
14.820831	1141.705747	11.310592
14.945304	1145.655347	11.315597
14.809713	1153.123750	11.320602
14.674887	1159.432927	11.325607
15.077759	1159.099101	11.330611
15.064881	1157.476929	11.335616
14.861677	1155.635944	11.340621
15.313988	1154.079930	11.345626
15.215176	1154.942651	11.350631
15.202576	1166.406532	11.355635
15.338231	1155.871015	11.360640
15.195383	1157.141323	11.365645
15.497445	1157.274603	11.370650
14.914602	1171.882549	11.375655
15.172311	1174.131379	11.380659
15.263646	1184.080528	11.385664
15.276995	1186.929755	11.390669
15.708028	1193.052494	11.395674
15.518421	1198.854739	11.400679
15.669101	1186.430686	11.405683
15.511365	1197.976090	11.410688
15.587834	1187.468916	11.415693
15.832358	1204.783568	11.420698
15.887393	1209.558004	11.425703
16.378174	1208.666083	11.430707
16.401411	1197.762096	11.435712
16.371306	1186.626918	11.440717
16.406354	1186.071050	11.445722
16.301317	1170.576334	11.450727
16.317716	1184.768579	11.455731
16.099683	1180.832519	11.460736
16.270408	1184.703786	11.465741
16.359318	1186.047522	11.470746
16.173652	1183.421535	11.475751
16.364197	1185.507607	11.480755
16.406587	1181.197258	11.485760
16.373794	1201.151915	11.490765
16.527337	1199.127862	11.495770
16.744279	1205.429840	11.500775
16.838101	1203.016326	11.505779
16.558337	1196.820771	11.510784
16.831162	1203.187955	11.515789
16.971954	1208.204190	11.520794
16.746248	1212.208084	11.525799
17.021206	1201.834827	11.530803
17.130720	1212.487602	11.535808
16.847907	1214.597137	11.540813
17.082938	1204.544075	11.545818
16.956857	1223.389224	11.550823
17.130946	1206.200382	11.555827
16.865970	1218.125622	11.560832
17.201015	1206.359728	11.565837
17.283869	1215.652633	11.570842
17.033122	1220.754978	11.575847
17.203869	1222.139283	11.580851
17.036346	1219.037288	11.585856
17.182250	1213.852517	11.590861
17.271830	1212.953621	11.595866
17.181411	1207.238818	11.600871
17.236933	1207.592780	11.605875
17.407778	1221.109116	11.610880
17.618530	1239.247672	11.615885
17.639546	1230.480887	11.620890
17.414347	1250.907867	11.625895
18.001121	1235.984015	11.630899
18.024287	1244.835429	11.635904
17.777404	1246.537095	11.640909
18.190710	1248.830509	11.645914
18.338570	1239.455256	11.650919
18.246810	1227.173920	11.655923
17.879140	1223.990300	11.660928
17.922663	1222.876389	11.665933
18.140311	1223.199761	11.670938
18.193450	1236.990364	11.675943
18.381321	1232.079605	11.680947
18.315832	1234.029894	11.685952
18.247785	1225.118038	11.690957
17.815723	1223.707803	11.695962
18.096122	1235.796819	11.700967
18.324777	1240.321212	11.705971
18.147835	1251.489659	11.710976
18.205757	1251.892127	11.715981
18.269892	1245.335757	11.720986
18.556220	1252.126607	11.725991
18.506051	1256.654474	11.730995
18.552147	1262.695131	11.736000
18.418576	1263.412007	11.741005
18.816102	1271.196005	11.746010
18.614271	1286.916606	11.751015
18.793000	1281.120996	11.756019
18.486111	1293.914042	11.761024
18.857099	1284.187765	11.766029
19.128653	1290.031615	11.771034
18.708806	1287.304181	11.776039
18.918470	1289.901332	11.781043
18.681749	1288.483590	11.786048
18.741111	1284.249355	11.791053
18.934185	1284.966175	11.796058
18.873016	1313.528223	11.801063
19.443200	1307.783713	11.806067
19.362638	1320.289936	11.811072
19.290147	1319.339608	11.816077
19.792083	1322.442111	11.821082
19.329503	1327.964653	11.826087
19.551367	1316.992625	11.831091
19.766655	1309.842807	11.836096
19.680369	1300.318770	11.841101
19.772899	1317.058527	11.846106
19.768370	1315.065979	11.851111
20.120541	1308.066227	11.856115
20.079596	1298.616965	11.861120
19.521050	1294.802997	11.866125
19.923189	1291.919224	11.871130
19.705843	1300.441584	11.876135
20.126960	1301.962592	11.881139
19.893775	1318.517747	11.886144
19.975283	1311.431846	11.891149
20.455054	1307.594199	11.896154
20.175253	1322.321125	11.901159
20.157861	1305.430803	11.906163
20.306513	1313.281328	11.911168
20.462649	1315.931179	11.916173
20.083830	1305.069160	11.921178
19.998111	1306.965912	11.926183
20.223347	1310.535191	11.931187
20.111284	1309.364082	11.936192
20.478611	1306.421201	11.941197
20.309186	1307.422933	11.946202
19.907373	1309.294405	11.951207
20.412101	1306.943075	11.956211
20.484233	1316.518466	11.961216
20.224082	1321.122425	11.966221
20.619793	1334.122006	11.971226
20.855500	1341.477665	11.976231
20.896517	1346.617101	11.981235
21.085443	1347.482828	11.986240
21.478399	1341.326579	11.991245
21.272023	1331.996726	11.996250
21.068119	1333.658429	12.001255
20.995610	1311.854958	12.006259
21.025741	1308.928009	12.011264
21.168557	1302.286520	12.016269
21.228118	1300.208055	12.021274
21.010198	1315.737277	12.026279
21.501814	1312.380312	12.031283
21.342676	1308.848006	12.036288
21.069706	1313.222183	12.041293
21.221026	1305.978486	12.046298
20.988015	1311.213658	12.051303
21.004565	1304.300556	12.056307
20.968112	1301.554548	12.061312
21.323926	1325.882014	12.066317
21.229519	1324.977762	12.071322
20.815772	1316.680835	12.076327
21.186058	1322.764431	12.081331
21.531232	1338.653321	12.086336
21.043210	1328.679226	12.091341
21.291630	1313.090134	12.096346
20.957787	1316.360634	12.101351
21.410869	1318.579904	12.106355
21.400233	1322.155265	12.111360
21.221503	1311.464765	12.116365
20.934585	1307.498654	12.121370
21.126003	1308.272513	12.126375
21.423731	1312.538318	12.131379
21.104996	1311.338669	12.136384
21.042516	1313.640168	12.141389
21.303218	1313.827359	12.146394
20.980962	1317.963381	12.151399
21.137240	1313.032401	12.156403
20.985210	1311.011337	12.161408
21.350177	1309.190103	12.166413
21.252623	1311.825220	12.171418
21.134270	1315.271096	12.176423
21.381183	1317.930123	12.181427
21.507987	1323.268768	12.186432
21.402368	1317.245669	12.191437
21.336017	1314.357763	12.196442
21.257686	1317.341493	12.201447
21.429893	1311.608416	12.206451
21.052495	1319.467151	12.211456
21.078736	1324.889648	12.216461
21.425460	1316.323187	12.221466
21.372410	1323.985105	12.226471
21.444593	1323.659864	12.231475
21.162557	1319.664584	12.236480
21.246252	1315.405957	12.241485
21.546506	1319.529429	12.246490
20.981807	1315.203900	12.251495
21.038353	1316.464496	12.256499
21.438923	1313.508426	12.261504
21.440780	1304.295196	12.266509
21.595135	1293.680900	12.271514
21.036642	1282.409140	12.276519
21.171084	1289.684726	12.281523
21.198044	1279.280003	12.286528
21.263367	1290.577005	12.291533
21.297700	1283.738351	12.296538
20.905399	1294.527998	12.301543
21.206237	1291.624111	12.306547
21.099224	1291.396841	12.311552
21.148753	1277.500124	12.316557
21.388206	1282.864944	12.321562
21.292010	1300.634622	12.326567
21.703117	1281.715730	12.331571
21.398056	1284.358705	12.336576
21.106979	1287.922015	12.341581
21.696725	1291.852641	12.346586
21.389142	1290.949274	12.351591
21.319223	1289.784061	12.356595
21.185494	1296.878485	12.361600
21.052073	1289.995618	12.366605
21.051349	1274.868948	12.371610
21.293897	1293.966069	12.376615
21.238751	1285.154624	12.381619
21.271763	1286.458398	12.386624
21.007648	1272.504473	12.391629
21.448309	1284.946456	12.396634
21.123186	1290.970635	12.401639
20.678576	1276.627581	12.406643
20.888466	1287.485187	12.411648
21.155736	1288.773675	12.416653
21.565959	1294.526021	12.421658
21.419108	1296.938751	12.426663
21.154935	1283.071561	12.431667
21.153437	1272.802276	12.436672
21.380040	1274.302263	12.441677
21.492519	1264.503684	12.446682
21.280597	1266.032611	12.451687
21.360490	1269.990932	12.456691
21.194255	1272.297934	12.461696
21.597892	1274.520352	12.466701
21.455980	1273.134800	12.471706
21.033076	1281.167938	12.476711
21.446012	1276.667566	12.481715
21.270688	1269.412905	12.486720
20.770070	1269.929691	12.491725
21.210013	1274.861965	12.496730
21.320734	1278.779099	12.501735
21.265063	1270.762571	12.506739
21.294175	1264.467257	12.511744
21.321886	1275.030619	12.516749
21.349411	1268.681937	12.521754
21.313951	1281.624079	12.526759
21.459640	1270.631117	12.531763
21.247102	1253.443958	12.536768
20.884147	1251.699406	12.541773
21.192467	1254.652995	12.546778
21.119331	1263.273763	12.551783
21.027214	1269.951509	12.556787
21.179426	1282.232906	12.561792
20.933990	1270.680977	12.566797
21.200243	1280.878274	12.571802
20.772190	1285.661974	12.576807
21.198552	1271.872324	12.581811
21.177995	1261.005238	12.586816
20.996678	1284.937312	12.591821
21.200836	1284.829154	12.596826
21.001385	1276.061233	12.601831
20.964982	1274.466455	12.606835
21.149652	1275.638800	12.611840
20.941587	1272.552721	12.616845
21.145586	1273.914381	12.621850
20.902674	1281.871500	12.626855
21.045434	1275.315192	12.631859
21.273083	1271.546153	12.636864
21.082484	1276.383445	12.641869
21.198793	1276.746638	12.646874
21.163700	1275.623183	12.651879
21.388363	1275.150615	12.656883
21.121239	1274.351188	12.661888
21.043371	1288.914979	12.666893
21.259675	1282.686000	12.671898
21.221495	1281.326482	12.676903
21.033996	1276.554430	12.681907
21.446834	1282.028796	12.686912
21.228204	1276.528390	12.691917
21.464599	1284.070000	12.696922
21.209677	1284.432476	12.701927
21.278699	1275.388334	12.706931
21.218628	1278.951068	12.711936
20.988586	1279.689640	12.716941
21.588219	1273.550920	12.721946
21.184865	1286.348306	12.726951
21.091540	1282.576840	12.731955
21.330066	1286.889929	12.736960
21.176111	1290.240548	12.741965
21.450459	1285.718121	12.746970
21.153993	1280.253782	12.751975
21.506032	1274.686012	12.756979
21.069500	1270.209160	12.761984
20.997593	1267.143946	12.766989
21.206044	1272.813342	12.771994
20.750210	1282.845100	12.776999
21.467783	1282.224524	12.782003
21.471909	1279.399505	12.787008
20.889046	1271.892860	12.792013
21.097290	1274.192176	12.797018
20.969251	1289.856853	12.802023
21.372913	1294.496860	12.807027
21.473233	1292.066524	12.812032
21.086281	1272.645696	12.817037
21.348809	1259.013083	12.822042
21.218862	1248.095642	12.827047
21.125669	1251.491756	12.832051
21.238341	1249.996212	12.837056
21.294342	1249.626242	12.842061
21.557395	1254.848509	12.847066
21.160034	1259.796047	12.852071
21.140659	1260.646104	12.857075
21.062771	1254.363130	12.862080
21.035727	1259.464503	12.867085
21.204364	1259.141226	12.872090
20.933998	1262.027835	12.877095
20.952190	1263.679339	12.882099
21.336920	1267.529112	12.887104
21.162607	1259.971504	12.892109
21.198656	1257.901525	12.897114
20.882442	1263.936889	12.902119
21.076754	1260.326142	12.907123
21.047613	1267.378637	12.912128
21.324536	1271.234566	12.917133
21.458447	1259.664721	12.922138
21.051557	1263.084062	12.927143
21.297131	1259.174966	12.932147
21.372783	1251.137503	12.937152
21.174191	1258.259601	12.942157
21.735588	1252.335156	12.947162
21.452766	1260.582494	12.952167
21.494545	1254.744079	12.957171
21.548863	1259.381445	12.962176
21.408332	1250.990513	12.967181
21.431156	1265.273280	12.972186
21.369626	1244.029582	12.977191
21.385261	1232.363500	12.982195
21.353154	1240.223893	12.987200
21.033460	1230.655123	12.992205
21.247814	1220.010809	12.997210
20.746057	1227.165475	13.002215
21.103973	1228.658707	13.007219
21.336225	1235.108074	13.012224
20.908616	1242.902234	13.017229
21.404687	1229.109391	13.022234
21.191566	1238.596181	13.027239
21.091767	1238.492347	13.032243
20.999963	1236.100549	13.037248
21.143859	1233.962907	13.042253
20.978785	1234.512911	13.047258
20.930649	1249.467755	13.052263
21.421255	1257.463992	13.057267
21.365724	1251.691564	13.062272
21.170178	1251.743357	13.067277
21.419865	1240.374268	13.072282
21.408221	1233.196025	13.077287
21.488597	1230.281579	13.082291
21.440425	1236.693668	13.087296
20.797320	1243.094990	13.092301
21.168951	1240.999875	13.097306
20.971223	1240.673529	13.102311
21.100643	1235.907716	13.107315
21.034422	1242.649131	13.112320
20.792214	1242.170599	13.117325
20.758219	1252.893605	13.122330
20.949479	1261.275073	13.127335
20.997074	1278.554990	13.132339
21.343555	1277.723930	13.137344
21.119178	1279.702722	13.142349
21.293797	1280.140197	13.147354
21.262695	1287.707127	13.152359
21.032226	1278.038935	13.157363
21.193516	1279.022612	13.162368
21.210048	1286.873695	13.167373
21.378891	1277.641734	13.172378
21.307797	1280.712616	13.177383
21.434290	1273.013979	13.182387
21.158208	1256.313214	13.187392
21.310478	1256.225948	13.192397
21.083824	1243.234372	13.197402
21.006826	1258.935032	13.202407
20.967332	1255.883574	13.207411
21.059901	1251.688209	13.212416
21.188376	1277.829165	13.217421
21.510239	1267.631317	13.222426
21.498365	1269.398009	13.227431
21.549707	1245.385966	13.232435
21.268395	1243.978494	13.237440
21.263146	1256.586196	13.242445
21.224668	1247.081378	13.247450
21.181128	1246.476537	13.252455
21.370124	1247.235009	13.257459
21.413547	1252.415031	13.262464
20.996770	1257.305738	13.267469
21.202138	1238.172123	13.272474
21.136212	1242.010185	13.277479
20.799613	1259.281967	13.282483
21.068277	1254.773072	13.287488
21.161907	1252.654485	13.292493
21.239997	1247.064183	13.297498
20.915343	1254.834043	13.302503
20.904769	1247.262942	13.307507
21.138827	1247.291948	13.312512
20.842663	1257.336070	13.317517
21.142396	1251.193150	13.322522
20.883524	1259.998090	13.327527
21.037466	1243.869026	13.332531
21.297344	1255.128661	13.337536
20.899977	1257.628651	13.342541
21.086249	1263.743149	13.347546
21.317125	1285.788012	13.352551
21.315993	1288.472404	13.357555
21.087181	1266.469992	13.362560
20.887250	1260.884603	13.367565
21.242501	1262.729941	13.372570
21.253963	1289.316956	13.377575
21.288981	1283.897522	13.382579
21.167989	1268.007834	13.387584
20.782560	1269.614900	13.392589
21.571423	1269.050767	13.397594
21.302374	1268.712140	13.402599
21.276864	1256.752965	13.407603
21.277830	1264.857267	13.412608
21.004901	1264.257472	13.417613
21.289638	1256.273394	13.422618
21.125186	1260.794259	13.427623
21.384505	1252.022569	13.432627
21.082838	1256.894916	13.437632
20.980212	1253.706865	13.442637
21.534832	1255.591369	13.447642
21.060942	1256.137010	13.452647
21.060806	1264.681478	13.457651
21.134246	1261.224057	13.462656
21.297822	1259.971141	13.467661
21.412813	1251.277667	13.472666
21.166804	1257.787556	13.477671
21.295244	1256.962887	13.482675
21.170724	1261.155669	13.487680
21.160270	1253.403187	13.492685
21.396632	1253.625800	13.497690
21.301274	1263.986422	13.502695
21.084181	1262.297456	13.507699
21.335754	1261.579311	13.512704
21.390578	1265.450161	13.517709
21.283409	1274.055863	13.522714
21.026323	1270.331021	13.527719
21.363059	1270.755255	13.532723
21.399771	1268.910684	13.537728
20.958651	1262.788147	13.542733
21.254692	1261.011031	13.547738
20.920203	1270.174984	13.552743
20.964025	1260.012025	13.557747
21.276398	1265.420404	13.562752
21.045697	1272.068212	13.567757
21.096920	1262.973297	13.572762
20.952683	1267.566637	13.577767
21.271811	1260.283581	13.582771
21.154147	1279.879704	13.587776
21.018800	1277.144743	13.592781
21.553712	1269.590712	13.597786
21.384913	1268.416040	13.602791
21.305084	1268.756896	13.607795
21.393026	1261.747268	13.612800
21.229148	1262.940510	13.617805
21.160857	1269.133461	13.622810
20.714863	1265.486062	13.627815
20.864276	1263.585667	13.632819
21.191139	1265.460766	13.637824
20.909473	1264.591116	13.642829
21.270968	1261.888882	13.647834
21.089914	1267.000628	13.652839
21.247105	1264.370406	13.657843
21.331130	1263.295765	13.662848
21.081380	1273.015512	13.667853
21.218419	1261.618640	13.672858
21.210093	1273.976100	13.677863
21.030623	1263.178515	13.682867
20.934748	1265.726619	13.687872
20.834486	1272.465592	13.692877
21.048699	1270.632136	13.697882
21.157619	1278.504750	13.702887
21.122093	1275.581972	13.707891
21.347285	1270.622667	13.712896
21.007279	1277.092360	13.717901
21.326589	1259.708396	13.722906
21.078335	1272.074158	13.727911
21.147836	1263.531443	13.732915
21.743174	1265.130320	13.737920
20.917997	1269.844885	13.742925
21.305350	1259.895229	13.747930
21.306913	1272.005094	13.752935
21.062373	1264.007654	13.757939
20.814674	1270.621902	13.762944
20.982875	1280.782796	13.767949
21.264506	1270.137177	13.772954
20.616428	1276.704894	13.777959
21.101129	1271.541764	13.782963
21.385013	1275.902811	13.787968
20.789469	1274.103887	13.792973
21.198378	1280.616565	13.797978
21.088172	1271.717712	13.802983
21.244535	1278.937754	13.807987
21.314653	1285.425620	13.812992
21.226018	1275.775811	13.817997
21.586918	1271.520295	13.823002
21.532955	1274.426009	13.828007
21.366790	1275.398832	13.833011
21.395997	1268.959992	13.838016
21.268032	1280.828736	13.843021
21.207269	1282.984870	13.848026
21.270910	1283.320191	13.853031
21.124585	1288.620381	13.858035
21.264779	1279.812478	13.863040
21.206894	1282.520114	13.868045
21.034218	1276.165511	13.873050
21.149667	1275.374454	13.878055
21.123480	1287.775778	13.883059
21.116092	1272.921423	13.888064
21.185764	1280.084326	13.893069
21.516585	1278.419938	13.898074
21.341692	1274.196259	13.903079
21.477042	1276.412580	13.908083
21.595311	1249.243679	13.913088
21.168932	1249.032653	13.918093
21.364964	1244.043314	13.923098
21.098138	1244.022893	13.928103
20.718701	1248.831944	13.933107
20.772769	1250.162320	13.938112
20.785438	1270.008890	13.943117
21.256281	1274.789571	13.948122
21.108723	1278.273214	13.953127
21.249164	1280.143354	13.958131
21.321095	1281.428303	13.963136
21.052550	1275.413861	13.968141
21.345125	1275.204864	13.973146
21.511010	1280.278626	13.978151
21.447201	1262.487386	13.983155
21.569528	1258.645259	13.988160
21.046143	1255.584244	13.993165
21.156041	1254.607984	13.998170
21.254308	1246.691502	14.003175
21.277336	1247.157885	14.008179
21.114760	1251.290499	14.013184
21.085640	1254.625929	14.018189
21.295458	1244.223078	14.023207
21.190984	1256.493553	14.028224
21.052051	1258.500948	14.033242
21.074457	1258.598149	14.038259
21.230510	1249.745655	14.043277
21.355581	1236.386732	14.048295
21.247095	1254.735933	14.053312
21.286121	1250.476405	14.058330
21.144917	1243.675334	14.063347
21.045641	1254.194225	14.068365
20.801840	1250.948777	14.073383
21.022524	1265.440391	14.078400
21.335949	1281.513831	14.083418
21.713124	1283.069255	14.088435
21.165368	1292.020629	14.093453
21.156847	1291.204125	14.098471
21.265786	1290.038555	14.103488
21.157291	1292.476824	14.108506
21.228458	1294.642621	14.113523
21.056648	1298.689167	14.118541
21.401633	1296.343943	14.123559
21.434844	1299.670384	14.128576
21.108917	1302.033223	14.133594
21.751905	1302.632333	14.138611
21.764832	1320.767199	14.143629
21.967698	1313.259991	14.148647
21.428125	1301.237113	14.153664
21.833626	1302.748695	14.158682
21.693004	1297.515799	14.163699
21.345779	1299.073507	14.168717
21.474637	1309.376728	14.173735
21.743983	1310.164420	14.178752
21.727369	1325.285394	14.183770
22.005228	1321.749090	14.188787
21.597654	1330.221955	14.193805
22.131502	1328.365697	14.198823
21.915412	1327.229943	14.203840
21.960498	1311.338574	14.208858
21.770946	1303.068129	14.213875
21.551699	1311.614764	14.218893
22.006638	1319.069168	14.223911
22.146325	1327.665529	14.228928
21.881011	1325.162813	14.233946
21.726392	1305.611440	14.238963
22.067741	1311.227805	14.243981
22.143362	1318.895291	14.248999
22.172093	1320.433936	14.254016
21.635665	1310.995008	14.259034
21.805411	1309.569629	14.264051
21.746283	1318.057697	14.269069
22.350732	1325.603088	14.274087
21.971489	1332.797295	14.279104
21.859797	1331.504891	14.284122
21.848894	1325.721189	14.289139
21.837082	1339.691539	14.294157
21.860345	1326.241808	14.299175
22.065099	1331.798170	14.304192
21.712581	1334.025257	14.309210
22.036827	1325.130160	14.314227
22.104984	1342.881867	14.319245
22.315383	1344.787940	14.324263
22.461883	1350.410228	14.329280
22.249981	1342.928261	14.334298
22.115657	1342.850687	14.339315
22.149183	1349.375029	14.344333
22.321105	1353.228341	14.349351
22.438021	1365.702696	14.354368
22.292020	1367.391910	14.359386
22.638484	1366.485751	14.364403
22.787867	1359.166373	14.369421
22.289986	1350.116098	14.374439
22.447191	1352.994915	14.379456
22.506006	1365.302358	14.384474
22.460548	1356.752498	14.389491
22.439382	1365.294313	14.394509
22.553436	1356.379240	14.399527
22.491050	1358.778705	14.404544
22.246614	1366.289626	14.409562
22.621572	1355.283298	14.414579
22.566528	1361.257059	14.419597
22.559480	1366.784296	14.424615
22.661709	1363.535542	14.429632
22.581305	1358.934810	14.434650
22.627827	1354.343722	14.439667
22.403434	1365.785560	14.444685
22.532198	1365.208276	14.449703
22.384337	1362.365924	14.454720
22.311190	1371.268389	14.459738
22.554796	1370.635037	14.464755
22.368899	1382.548945	14.469773
22.392057	1392.532457	14.474791
22.808273	1376.589688	14.479808
22.444708	1389.426988	14.484826
22.973507	1390.325886	14.489843
22.887421	1388.208276	14.494861
22.805119	1393.832469	14.499879
22.950077	1396.894145	14.504896
22.669199	1387.345195	14.509914
23.079144	1391.929760	14.514931
23.053118	1393.135801	14.519949
22.916308	1394.373669	14.524967
22.977184	1394.983832	14.529984
23.089968	1390.443512	14.535002
23.014974	1387.444815	14.540019
23.115843	1388.709267	14.545037
23.304348	1387.038644	14.550055
23.558100	1389.409714	14.555072
23.214052	1389.823339	14.560090
23.653758	1386.067724	14.565107
23.612021	1389.028615	14.570125
23.561197	1378.807477	14.575143
23.589690	1388.057109	14.580160
23.394511	1380.959417	14.585178
23.555405	1354.975917	14.590195
23.311113	1351.241317	14.595213
23.436768	1354.150334	14.600231
23.116191	1350.851043	14.605248
23.193391	1353.676553	14.610266
23.547073	1345.511348	14.615283
23.301855	1361.554429	14.620301
23.231722	1357.315426	14.625319
23.453491	1349.345863	14.630336
23.013768	1356.298045	14.635354
23.194848	1362.202686	14.640371
23.113348	1376.412274	14.645389
23.520846	1377.355687	14.650407
23.742026	1373.954252	14.655424
23.582391	1385.274092	14.660442
23.677395	1373.374883	14.665459
23.837543	1384.047545	14.670477
23.694131	1385.487811	14.675495
23.710403	1388.755627	14.680512
23.658746	1379.796184	14.685530
23.721021	1374.611121	14.690547
23.797779	1390.357489	14.695565
23.746674	1383.013448	14.700583
23.973193	1381.322605	14.705600
23.591573	1374.960938	14.710618
23.733585	1361.662120	14.715635
23.766710	1367.569911	14.720653
23.590442	1377.141630	14.725671
23.837597	1371.134280	14.730688
23.913126	1378.943384	14.735706
23.868157	1381.900069	14.740723
24.091384	1382.748605	14.745741
24.038707	1376.559414	14.750759
24.245785	1377.375918	14.755776
23.704861	1372.285492	14.760794
23.829423	1370.725742	14.765811
23.882852	1388.744121	14.770829
23.664230	1390.215261	14.775847
23.846057	1385.188878	14.780864
23.901629	1387.711106	14.785882
23.986822	1378.427816	14.790899
24.098473	1382.956136	14.795917
24.066823	1379.208063	14.800935
24.266888	1372.275423	14.805952
24.082442	1377.086920	14.810970
24.040116	1384.615951	14.815987
24.446586	1382.221581	14.821005
24.236663	1382.760105	14.826023
23.936608	1385.114111	14.831040
24.002682	1385.198056	14.836058
24.020871	1390.461728	14.841075
23.982520	1385.841696	14.846093
23.948952	1392.350017	14.851111
24.667291	1404.975446	14.856128
24.419449	1401.716451	14.861146
24.069316	1391.745963	14.866163
24.384192	1404.405854	14.871181
23.971661	1421.603544	14.876199
24.347784	1418.639855	14.881216
24.404927	1420.007238	14.886234
24.533167	1419.000601	14.891251
24.677314	1419.617933	14.896269
24.648123	1420.719089	14.901287
24.845634	1411.532695	14.906304
24.345238	1425.881503	14.911322
24.775562	1413.071481	14.916339
24.975373	1420.000341	14.921357
24.633188	1411.460023	14.926375
24.768860	1397.968701	14.931392
24.390693	1394.947571	14.936410
24.441675	1398.299515	14.941427
24.397283	1417.532174	14.946445
24.390020	1420.934311	14.951463
24.544015	1411.529916	14.956480
24.702038	1414.397603	14.961498
24.546091	1422.578704	14.966515
24.952987	1418.317081	14.971533
24.817726	1414.755411	14.976551
24.843812	1420.304124	14.981568
25.031178	1427.713172	14.986586
24.909920	1421.309958	14.991603
24.888443	1413.173091	14.996621
24.816230	1416.983562	15.001639
24.872376	1412.512043	15.006656
24.818537	1421.557750	15.011674
24.799066	1431.206742	15.016691
24.955025	1427.403565	15.021709
24.616142	1422.435052	15.026727
24.853633	1429.847118	15.031744
25.169286	1453.582598	15.036762
24.929265	1449.498079	15.041779
25.253678	1441.586027	15.046797
25.058493	1456.542137	15.051815
25.455160	1448.181256	15.056832
25.323389	1447.906646	15.061850
25.163970	1447.872400	15.066867
25.360026	1445.790006	15.071885
25.393759	1442.202948	15.076903
25.726480	1438.854494	15.081920
25.629488	1442.234768	15.086938
25.338755	1431.683769	15.091955
25.290748	1433.118262	15.096973
25.283674	1412.959620	15.101991
25.478615	1417.466801	15.107008
25.475895	1422.560788	15.112026
25.230855	1426.079502	15.117043
25.527458	1430.905527	15.122061
25.280511	1436.088807	15.127079
25.479386	1444.436698	15.132096
25.763254	1441.608842	15.137114
25.734207	1435.140577	15.142131
25.730375	1429.668737	15.147149
25.200497	1431.107727	15.152167
25.669245	1429.909927	15.157184
25.401979	1443.828313	15.162202
25.695224	1452.516660	15.167219
25.719190	1442.903321	15.172237
25.704353	1451.654963	15.177255
25.794818	1441.735289	15.182272
25.633941	1446.359006	15.187290
25.762559	1454.582828	15.192307
25.949487	1441.832051	15.197325
25.750328	1454.234198	15.202343
25.744039	1443.909957	15.207360
25.945050	1446.572593	15.212378
25.664702	1448.460996	15.217395
25.988865	1440.931230	15.222413
25.870230	1446.476295	15.227431
25.958355	1452.353326	15.232448
25.854381	1449.159464	15.237466
25.970168	1437.623403	15.242483
25.949677	1439.017328	15.247501
26.059557	1443.781903	15.252519
26.068816	1442.975140	15.257536
26.233855	1438.892086	15.262554
26.034454	1441.859257	15.267571
26.212460	1442.626920	15.272589
25.857845	1439.440002	15.277607
26.028252	1439.472701	15.282624
25.634360	1443.120553	15.287642
25.946056	1436.105584	15.292659
25.957821	1440.077272	15.297677
25.797417	1468.483514	15.302695
26.602934	1473.989730	15.307712
26.318547	1469.745540	15.312730
26.165857	1470.539207	15.317747
26.405403	1480.966468	15.322765
26.391104	1468.079449	15.327783
26.372082	1463.572713	15.332800
26.360668	1483.062894	15.337818
26.295704	1490.590872	15.342835
26.375534	1479.634669	15.347853
26.426591	1482.873362	15.352871
26.691810	1477.679490	15.357888
26.754385	1476.942872	15.362906
26.344265	1473.325925	15.367923
26.631612	1472.578625	15.372941
26.750815	1475.468247	15.377959
26.899448	1474.192512	15.382976
26.840782	1468.501314	15.387994
26.593215	1483.195244	15.393011
26.808631	1478.734483	15.398029
26.710517	1481.361463	15.403047
26.798341	1482.794746	15.408064
27.088110	1474.705730	15.413082
26.456307	1477.439853	15.418099
26.881584	1480.862679	15.423117
26.314243	1480.256418	15.428135
26.819892	1473.378811	15.433152
26.671712	1463.662353	15.438170
26.575860	1471.439066	15.443187
26.973980	1469.458148	15.448205
26.684365	1469.458825	15.453223
26.705719	1476.052806	15.458240
26.992276	1470.378905	15.463258
27.091492	1469.251052	15.468275
26.923978	1468.003719	15.473293
27.079158	1478.858141	15.478311
27.530263	1479.901572	15.483328
27.440575	1474.662060	15.488346
27.008620	1466.150185	15.493363
27.351076	1463.983090	15.498381
27.184638	1470.904323	15.503399
27.086033	1471.826217	15.508416
27.202162	1462.223334	15.513434
26.942684	1460.661906	15.518451
27.063296	1466.318257	15.523469
27.272652	1480.840208	15.528487
27.438793	1487.338742	15.533504
27.871157	1492.278416	15.538522
27.441650	1489.853768	15.543539
27.782131	1464.956707	15.548557
27.642688	1467.727131	15.553575
27.608549	1464.073814	15.558592
27.572432	1465.868210	15.563610
27.104349	1470.443404	15.568627
27.071409	1468.649215	15.573645
27.590482	1479.412566	15.578663
27.271807	1479.340798	15.583680
27.319969	1477.167157	15.588698
27.437264	1506.222888	15.593715
27.883656	1491.134057	15.598733
27.781849	1490.780734	15.603751
27.900987	1494.994862	15.608768
27.972643	1491.524440	15.613786
28.007375	1490.100129	15.618803
27.939817	1473.380257	15.623821
27.934316	1467.985748	15.628839
27.809626	1464.327997	15.633856
27.704722	1463.767529	15.638874
27.680609	1462.074180	15.643891
28.059299	1466.262633	15.648909
27.821180	1469.086548	15.653927
27.642426	1479.967490	15.658944
28.059221	1481.548079	15.663962
28.157280	1489.525109	15.668979
28.227362	1485.990445	15.673997
28.262207	1484.393083	15.679015
27.948393	1473.279444	15.684032
28.152841	1462.163378	15.689050
27.642244	1472.350054	15.694067
27.898399	1478.442542	15.699085
28.073474	1487.332230	15.704103
28.054129	1489.438560	15.709120
28.532990	1485.182744	15.714138
27.981216	1486.705455	15.719155
28.187952	1492.948978	15.724173
27.884458	1483.348515	15.729191
28.194190	1492.792458	15.734208
28.185856	1491.691194	15.739226
27.999965	1498.684756	15.744243
28.226654	1495.523089	15.749261
28.559640	1480.759097	15.754279
27.809043	1487.070363	15.759296
28.162462	1502.598121	15.764314
28.212416	1514.859914	15.769331
28.413441	1521.181438	15.774349
28.457691	1521.261000	15.779367
28.565737	1533.707027	15.784384
28.664390	1519.958799	15.789402
28.399434	1524.243634	15.794419
28.754619	1521.171579	15.799437
29.203355	1516.012919	15.804455
28.853577	1523.860047	15.809472
28.776358	1523.002577	15.814490
28.666180	1519.405419	15.819507
28.949707	1520.779178	15.824525
29.033445	1510.029969	15.829543
28.629440	1500.812041	15.834560
28.605947	1493.279495	15.839578
28.705068	1516.797930	15.844595
28.624758	1515.723875	15.849613
28.803932	1509.827985	15.854631
28.777445	1522.756359	15.859648
29.099888	1510.493571	15.864666
28.924751	1518.341157	15.869683
28.997815	1515.189831	15.874701
29.278059	1517.863438	15.879719
29.125061	1521.568843	15.884736
29.337608	1512.884931	15.889754
29.173549	1523.549630	15.894771
29.275548	1520.657957	15.899789
29.409209	1510.220111	15.904807
29.029771	1522.578711	15.909824
29.569931	1513.655356	15.914842
29.407790	1514.061992	15.919859
29.145871	1516.192858	15.924877
29.458415	1511.579741	15.929895
29.112826	1515.528221	15.934912
29.489584	1511.625312	15.939930
29.079443	1516.601840	15.944947
29.302516	1520.146589	15.949965
29.322422	1513.008235	15.954983
28.890807	1518.672458	15.960000
29.703752	1509.276160	15.965018
29.425624	1500.439279	15.970035
29.450960	1516.925447	15.975053
29.348601	1514.956706	15.980071
29.318590	1512.399123	15.985088
29.588685	1514.525360	15.990106
29.344597	1515.365067	15.995123
29.119940	1512.490889	16.000141
29.517915	1520.541226	16.005159
29.327710	1532.842911	16.010176
29.739861	1531.666714	16.015194
29.719419	1557.486760	16.020211
29.806448	1547.875878	16.025229
30.300471	1537.808403	16.030247
30.158018	1553.711035	16.035264
29.846433	1531.861015	16.040282
29.771254	1529.137600	16.045299
29.802644	1532.775846	16.050317
30.360663	1542.123592	16.055335
29.974180	1536.977012	16.060352
30.216762	1515.866047	16.065370
30.110990	1523.966843	16.070387
30.135560	1509.763249	16.075405
30.125847	1509.525799	16.080423
29.747224	1507.173257	16.085440
30.045887	1516.243026	16.090458
29.681373	1532.939255	16.095475
29.950651	1541.205186	16.100493
30.132175	1536.652284	16.105511
30.137477	1543.066384	16.110528
30.290770	1538.411017	16.115546
30.381220	1541.994228	16.120563
30.307867	1540.176588	16.125581
30.459408	1538.176787	16.130599
30.185804	1544.533123	16.135616
30.392071	1536.792448	16.140634
30.338849	1540.000595	16.145651
30.204750	1550.596040	16.150669
30.535473	1539.267865	16.155687
30.175821	1546.144444	16.160704
30.064184	1545.983026	16.165722
30.276321	1545.272887	16.170739
30.277193	1562.074469	16.175757
30.630200	1568.436269	16.180775
30.688841	1578.563689	16.185792
30.686848	1572.754871	16.190810
30.725838	1574.678875	16.195827
30.731125	1568.865752	16.200845
31.234190	1569.603599	16.205863
31.051893	1577.271459	16.210880
30.901295	1550.385602	16.215898
30.934522	1545.115449	16.220915
30.906034	1534.124570	16.225933
30.822757	1535.092788	16.230951
30.669197	1545.771558	16.235968
30.973717	1548.420850	16.240986
30.803403	1552.633970	16.246003
30.672266	1563.639515	16.251021
30.865892	1561.577942	16.256039
31.320812	1575.236550	16.261056
30.978107	1571.132193	16.266074
31.139442	1570.219370	16.271091
31.451596	1560.078639	16.276109
31.477184	1557.809485	16.281127
30.987106	1551.587734	16.286144
31.064198	1557.033983	16.291162
31.287627	1562.494646	16.296179
31.204991	1566.166818	16.301197
31.558344	1564.657074	16.306215
31.550651	1572.385174	16.311232
31.638888	1557.271600	16.316250
31.269274	1541.260502	16.321267
30.836769	1542.138127	16.326285
31.030109	1557.660015	16.331303
31.055802	1568.706619	16.336320
31.162973	1564.105792	16.341338
31.049801	1569.942617	16.346355
30.968681	1570.092511	16.351373
31.072146	1569.882628	16.356391
31.290219	1592.034118	16.361408
31.421105	1595.603027	16.366426
31.593327	1597.796798	16.371443
31.682427	1598.526739	16.376461
32.009860	1593.414140	16.381479
31.918646	1597.831736	16.386496
31.840323	1593.744982	16.391514
32.249011	1595.377214	16.396531
31.958357	1590.808368	16.401549
32.051696	1597.367327	16.406567
32.029595	1598.748940	16.411584
31.846626	1592.731449	16.416602
31.687080	1590.427323	16.421619
31.840483	1607.659238	16.426637
32.134818	1595.117715	16.431655
32.058682	1598.741666	16.436672
32.105219	1596.582424	16.441690
32.252898	1593.085695	16.446707
31.586822	1601.159493	16.451725
31.993332	1592.614487	16.456743
31.781049	1591.810015	16.461760
32.011959	1583.488079	16.466778
32.058679	1592.075829	16.471795
32.033077	1587.736846	16.476813
32.323360	1589.911786	16.481831
32.038854	1598.080455	16.486848
32.209256	1598.132032	16.491866
32.342413	1599.487309	16.496883
32.257654	1606.375129	16.501901
32.333341	1618.853132	16.506919
32.545315	1624.521715	16.511936
32.508352	1622.695115	16.516954
32.540936	1624.525764	16.521971
32.529834	1620.267830	16.526989
32.707276	1621.903914	16.532007
32.619734	1619.533242	16.537024
32.670174	1613.911103	16.542042
32.664822	1615.640835	16.547059
32.542504	1612.058174	16.552077
32.689188	1613.744781	16.557095
32.811677	1621.464728	16.562112
32.677321	1621.418618	16.567130
33.030529	1612.784573	16.572147
32.897285	1624.529831	16.577165
33.025124	1611.893724	16.582183
33.126359	1617.513898	16.587200
32.837939	1599.757864	16.592218
32.944508	1586.271009	16.597235
32.939814	1591.906495	16.602253
32.842847	1596.465010	16.607271
33.046248	1605.323510	16.612288
33.550753	1605.117305	16.617306
33.468516	1592.258314	16.622323
32.862460	1581.663114	16.627341
32.939567	1573.612681	16.632359
33.368034	1586.934170	16.637376
32.951732	1595.103408	16.642394
33.464032	1611.263475	16.647411
33.089246	1611.656838	16.652429
33.237103	1610.343462	16.657447
33.232334	1618.541460	16.662464
33.210510	1612.152190	16.667482
33.625237	1616.891798	16.672499
33.342213	1630.161634	16.677517
33.687679	1616.108106	16.682535
33.187183	1620.759302	16.687552
32.937065	1618.474335	16.692570
33.371126	1614.744733	16.697587
33.303166	1618.230531	16.702605
33.294479	1615.213345	16.707623
33.304681	1610.528868	16.712640
33.464878	1621.145067	16.717658
33.673905	1642.307058	16.722675
33.454058	1645.609445	16.727693
33.904487	1645.259278	16.732711
34.157084	1651.860503	16.737728
33.807747	1644.318499	16.742746
34.310263	1641.007414	16.747763
33.921774	1632.755924	16.752781
33.667073	1612.911782	16.757799
33.923267	1629.988902	16.762816
33.988500	1637.480460	16.767834
34.150756	1633.953081	16.772851
33.982913	1639.315728	16.777869
34.061898	1630.870129	16.782887
33.950821	1632.305263	16.787904
33.906067	1644.733283	16.792922
34.117941	1634.630518	16.797939
33.928805	1646.527855	16.802957
33.999690	1652.807272	16.807975
33.943442	1649.572720	16.812992
34.110438	1641.312855	16.818010
34.343721	1640.426305	16.823027
34.198702	1644.283053	16.828045
34.011097	1647.736030	16.833063
34.162871	1644.163129	16.838080
34.188364	1648.162572	16.843098
34.422249	1636.563473	16.848115
34.228629	1651.579309	16.853133
34.520220	1659.129158	16.858151
34.424926	1667.277126	16.863168
34.694688	1673.600340	16.868186
34.595329	1671.980316	16.873203
34.624445	1676.614702	16.878221
34.466170	1669.929413	16.883239
34.577673	1667.346086	16.888256
34.607254	1672.502650	16.893274
35.122777	1666.637997	16.898291
34.773652	1667.346597	16.903309
35.108458	1660.875257	16.908327
35.134341	1665.510156	16.913344
34.962376	1663.639013	16.918362
35.030322	1667.021348	16.923379
34.881016	1663.897590	16.928397
35.251236	1665.024725	16.933415
35.464853	1655.959880	16.938432
35.120005	1647.736028	16.943450
34.992828	1627.009497	16.948467
35.021069	1631.746256	16.953485
34.937997	1629.950604	16.958503
35.404654	1640.547829	16.963520
35.077261	1651.207210	16.968538
35.264755	1652.319442	16.973555
35.400355	1658.553933	16.978573
35.224554	1652.695724	16.983591
35.477604	1650.039488	16.988608
35.139828	1664.178545	16.993626
35.284263	1660.701194	16.998643
35.333029	1667.416734	17.003661
35.296398	1663.861293	17.008679
35.440578	1666.896409	17.013696
35.513708	1661.199845	17.018714
35.500452	1657.755511	17.023731
35.686296	1665.043799	17.028749
35.458393	1667.070159	17.033767
35.792812	1662.414180	17.038784
35.597574	1662.726997	17.043802
35.607447	1654.864997	17.048819
35.585811	1665.343487	17.053837
35.223096	1670.715203	17.058855
35.536815	1658.217726	17.063872
35.514752	1668.115830	17.068890
35.678077	1680.122151	17.073907
35.899304	1682.805203	17.078925
36.072840	1680.567490	17.083943
36.141844	1684.797535	17.088960
36.189354	1689.740456	17.093978
35.895766	1671.228519	17.098995
35.879909	1679.075956	17.104013
35.780840	1669.664564	17.109031
35.854984	1682.032754	17.114048
35.866149	1689.364645	17.119066
36.321222	1686.891690	17.124083
36.264027	1691.215797	17.129101
35.936002	1685.677588	17.134119
36.048749	1684.885767	17.139136
35.985826	1688.087628	17.144154
36.274988	1684.623369	17.149171
36.095128	1691.037177	17.154189
35.968585	1703.651328	17.159207
36.453283	1712.647505	17.164224
36.653136	1723.214982	17.169242
36.746649	1707.461750	17.174259
36.477056	1707.721932	17.179277
36.625292	1719.315405	17.184295
36.844215	1714.465468	17.189312
36.825790	1717.627204	17.194330
36.825878	1709.891007	17.199347
36.889116	1705.706136	17.204365
36.644911	1705.477768	17.209383
36.929361	1700.578058	17.214400
36.947809	1703.002440	17.219418
36.848897	1692.126495	17.224435
36.834074	1700.856262	17.229453
36.809426	1704.871584	17.234471
37.221627	1703.654468	17.239488
37.016064	1717.157425	17.244506
37.071917	1713.137328	17.249523
37.083769	1702.276744	17.254541
36.992108	1702.466075	17.259559
37.035288	1706.621592	17.264576
37.045357	1705.813111	17.269594
37.349215	1705.813516	17.274611
36.906208	1706.645632	17.279629
36.584967	1701.851962	17.284647
37.175820	1706.824637	17.289664
37.100936	1708.548166	17.294682
37.234834	1703.887975	17.299699
37.064252	1706.043626	17.304717
37.275978	1714.550076	17.309735
36.958527	1724.839829	17.314752
37.374236	1736.684819	17.319770
37.405752	1734.010416	17.324787
37.494472	1730.420809	17.329805
37.565631	1738.737329	17.334823
37.460522	1727.448631	17.339840
37.517257	1733.118421	17.344858
37.652375	1730.285920	17.349875
37.635795	1731.877455	17.354893
37.466335	1733.556294	17.359911
37.903972	1728.106742	17.364928
37.465695	1726.669757	17.369946
37.723132	1724.723829	17.374963
37.397154	1736.905766	17.379981
37.717323	1758.747066	17.384999
37.710864	1753.579124	17.390016
37.971524	1757.777049	17.395034
38.109344	1759.427334	17.400051
38.059139	1756.835175	17.405069
38.048818	1764.868970	17.410087
38.250466	1754.344599	17.415104
38.337883	1761.305708	17.420122
38.327326	1754.996377	17.425139
38.420617	1765.308741	17.430157
38.156547	1766.996382	17.435175
38.191950	1758.431815	17.440192
38.267874	1760.755803	17.445210
38.224261	1764.100895	17.450227
38.387334	1759.343223	17.455245
38.332165	1767.947328	17.460263
38.583093	1750.138122	17.465280
38.399085	1757.932194	17.470298
38.015178	1762.322588	17.475315
38.377895	1761.355612	17.480333
38.610007	1783.080429	17.485351
39.103109	1775.682427	17.490368
39.141541	1764.979582	17.495386
38.818559	1761.590913	17.500403
39.141006	1757.934135	17.505421
38.857162	1758.951658	17.510439
38.734810	1744.384295	17.515456
38.813276	1750.207931	17.520474
39.053782	1749.416180	17.525491
38.904056	1746.921695	17.530509
38.717655	1752.214982	17.535527
38.847802	1753.240412	17.540544
38.998275	1762.673752	17.545562
38.955542	1780.613572	17.550579
39.345834	1772.171725	17.555597
39.465065	1776.261649	17.560615
39.316700	1765.579158	17.565632
38.932855	1769.872014	17.570650
39.054700	1763.873478	17.575667
39.329863	1774.279541	17.580685
39.112712	1782.058462	17.585703
39.341388	1780.813981	17.590720
39.554983	1775.467786	17.595738
39.430252	1789.006682	17.600755
39.746516	1775.119684	17.605773
39.754902	1776.861402	17.610791
39.951957	1763.498381	17.615808
39.585455	1781.941308	17.620826
39.609620	1778.152768	17.625843
39.882227	1764.253866	17.630861
39.676419	1757.296113	17.635879
39.486072	1763.666007	17.640896
39.571025	1770.687289	17.645914
39.534218	1769.845382	17.650931
39.804318	1764.645912	17.655949
39.246467	1772.853555	17.660967
39.656569	1773.603096	17.665984
39.542062	1779.002906	17.671002
39.618803	1773.963263	17.676019
39.935368	1777.996545	17.681037
39.851778	1795.357720	17.686055
40.103258	1806.119950	17.691072
40.323103	1802.331656	17.696090
40.358782	1800.701092	17.701107
40.089310	1799.540777	17.706125
40.243771	1800.483680	17.711143
40.265313	1793.319758	17.716160
40.475757	1796.426132	17.721178
40.705620	1800.737524	17.726195
40.851075	1801.850181	17.731213
40.346730	1787.788875	17.736231
40.203884	1774.867027	17.741248
40.474518	1789.687836	17.746266
40.328865	1789.596335	17.751283
40.437163	1794.325098	17.756301
40.667820	1798.659959	17.761319
40.959390	1807.488792	17.766336
40.434332	1806.432163	17.771354
40.553518	1808.140482	17.776371
41.168404	1804.905824	17.781389
40.866027	1807.044756	17.786407
40.704090	1793.644579	17.791424
40.828485	1797.261766	17.796442
40.636897	1801.835435	17.801459
40.855605	1788.744223	17.806477
40.755263	1802.084183	17.811495
40.694484	1803.259620	17.816512
41.056111	1797.828457	17.821530
40.695148	1799.297168	17.826547
40.878017	1816.005521	17.831565
40.661888	1827.133362	17.836583
40.774326	1832.940602	17.841600
40.948050	1826.751291	17.846618
41.024396	1822.311032	17.851635
41.426823	1828.572256	17.856653
41.397716	1830.766711	17.861671
41.275049	1822.798340	17.866688
41.322043	1819.951562	17.871706
41.307687	1837.773665	17.876723
41.420195	1854.502723	17.881741
41.330115	1859.643830	17.886759
41.526882	1862.647004	17.891776
41.830271	1858.472554	17.896794
41.935590	1854.241603	17.901811
42.158608	1864.028392	17.906829
41.687765	1861.679485	17.911847
41.917939	1841.021500	17.916864
41.840478	1833.167040	17.921882
41.676511	1828.966460	17.926899
42.175365	1836.149857	17.931917
41.766006	1833.756541	17.936935
41.740900	1847.038923	17.941952
41.991939	1848.674307	17.946970
42.103713	1850.589886	17.951987
42.600845	1861.608715	17.957005
42.185080	1855.442620	17.962023
42.283977	1832.762165	17.967040
42.498172	1827.739908	17.972058
42.084387	1829.600874	17.977075
42.334651	1810.357063	17.982093
42.019485	1819.617733	17.987111
41.894282	1837.544034	17.992128
42.812093	1840.904127	17.997146
42.450881	1848.869659	18.002163
42.607991	1851.927921	18.007181
42.319646	1853.628881	18.012199
42.374567	1852.248507	18.017216
42.173464	1855.307270	18.022234
42.239316	1853.291205	18.027251
42.355823	1852.936089	18.032269
42.544277	1851.384976	18.037287
42.432094	1860.610153	18.042304
42.708599	1864.091409	18.047322
42.530031	1869.761027	18.052339
43.181496	1872.375497	18.057357
42.833689	1885.757360	18.062375
42.820061	1885.325467	18.067392
42.928890	1870.875267	18.072410
43.016535	1871.370280	18.077427
43.246390	1872.025875	18.082445
43.115850	1871.084077	18.087463
42.755339	1873.084421	18.092480
43.073146	1871.572453	18.097498
43.184619	1869.044153	18.102515
43.302774	1860.066768	18.107533
42.926273	1875.268522	18.112551
43.209322	1868.837594	18.117568
43.426109	1859.888524	18.122586
43.292256	1866.416198	18.127603
43.331947	1866.059176	18.132621
43.367205	1876.093789	18.137639
43.569474	1884.242399	18.142656
43.924189	1883.169723	18.147674
43.652634	1899.857837	18.152691
43.795599	1897.396872	18.157709
43.905726	1890.783507	18.162727
43.768946	1882.140933	18.167744
43.852948	1864.878897	18.172762
43.560273	1871.910117	18.177779
43.806478	1878.424374	18.182797
43.999327	1884.919615	18.187815
43.826587	1886.655625	18.192832
44.111469	1892.153020	18.197850
44.086037	1897.353831	18.202867
44.341143	1870.778639	18.207885
43.903193	1877.390212	18.212903
43.895685	1889.739354	18.217920
44.231951	1893.341651	18.222938
44.275583	1891.914308	18.227955
44.029812	1895.263357	18.232973
44.350424	1891.955275	18.237991
44.189040	1893.637563	18.243008
44.440540	1892.130662	18.248026
44.269800	1888.385763	18.253043
44.317964	1880.092018	18.258061
44.139387	1882.096381	18.263079
44.454236	1888.745991	18.268096
44.631238	1882.497143	18.273114
44.638444	1886.029220	18.278131
44.711892	1884.758362	18.283149
45.102808	1879.073167	18.288167
44.702685	1889.626340	18.293184
44.872439	1883.333028	18.298202
44.803798	1884.166009	18.303219
44.882876	1881.715235	18.308237
44.774294	1875.681043	18.313255
44.763967	1895.974659	18.318272
45.043024	1885.797296	18.323290
44.722339	1893.607733	18.328307
44.937521	1904.247620	18.333325
45.192549	1912.099172	18.338343
45.153315	1912.483070	18.343360
45.289854	1913.634912	18.348378
45.088972	1915.127654	18.353395
45.110825	1912.393410	18.358413
45.534483	1913.459346	18.363431
45.010569	1921.669524	18.368448
45.066309	1908.022944	18.373466
45.104529	1913.570698	18.378483
45.367137	1909.937584	18.383501
45.321743	1911.078328	18.388519
45.419112	1925.021603	18.393536
45.502114	1932.553739	18.398554
45.841602	1937.407705	18.403571
45.666552	1930.389904	18.408589
46.047547	1942.191048	18.413607
45.829032	1949.569926	18.418624
46.152751	1934.209185	18.423642
46.055715	1936.407411	18.428659
45.892234	1933.912727	18.433677
46.315419	1939.375498	18.438695
45.995818	1936.963129	18.443712
46.113748	1918.528394	18.448730
46.099729	1918.688040	18.453747
46.138084	1931.383845	18.458765
46.080484	1930.189728	18.463783
46.086236	1940.824502	18.468800
46.386463	1930.429007	18.473818
46.126754	1936.512726	18.478835
46.217023	1933.035298	18.483853
46.243676	1934.055224	18.488871
46.402991	1937.456871	18.493888
46.366240	1931.626711	18.498906
46.149873	1939.426040	18.503923
46.254247	1935.406009	18.508941
46.412878	1927.590925	18.513959
46.099259	1938.167304	18.518976
46.247959	1947.849595	18.523994
46.464543	1951.468635	18.529011
46.433138	1962.042495	18.534029
46.602962	1958.097752	18.539047
46.489233	1965.984549	18.544064
46.680323	1959.222957	18.549082
46.589298	1980.493074	18.554099
46.900837	1988.492177	18.559117
47.217562	1993.534630	18.564135
47.029493	2000.111910	18.569152
47.499393	1996.060308	18.574170
47.219394	1996.126303	18.579187
47.582761	1997.887728	18.584205
47.898572	1982.263919	18.589223
47.506044	1973.946020	18.594240
47.178277	1964.297194	18.599258
47.639828	1953.293126	18.604275
47.611335	1953.328447	18.609293
47.932277	1950.759648	18.614311
47.634576	1959.267261	18.619328
47.863366	1950.521509	18.624346
47.826794	1946.870032	18.629363
47.569283	1945.942973	18.634381
47.527996	1950.661036	18.639399
47.291357	1963.442414	18.644416
47.716133	1944.447456	18.649434
47.722086	1953.553173	18.654451
47.740042	1968.976842	18.659469
47.999341	1969.140877	18.664487
47.876598	1980.882387	18.669504
48.210827	1988.811803	18.674522
47.941082	1995.393455	18.679539
48.038274	1990.003610	18.684557
48.248294	1981.518819	18.689575
48.015993	1984.050096	18.694592
48.311785	1979.157138	18.699610
48.359716	1992.047317	18.704627
48.176465	1980.295027	18.709645
48.362091	1979.366507	18.714663
47.980748	1989.629669	18.719680
48.244072	1982.471139	18.724698
48.210037	1977.426283	18.729715
47.958037	1993.876209	18.734733
48.485411	1988.513715	18.739751
48.395137	2007.418618	18.744768
48.824744	2003.162647	18.749786
48.659687	2020.204375	18.754803
48.729503	2014.637196	18.759821
49.093393	2008.261743	18.764839
48.954459	2011.451415	18.769856
48.901576	2008.008598	18.774874
49.112532	2018.937118	18.779891
48.938590	2012.682834	18.784909
48.816316	2017.586089	18.789927
48.756848	2011.868849	18.794944
49.009755	2011.917496	18.799962
48.683949	2013.996483	18.804979
48.664725	2011.014718	18.809997
48.957822	2021.233261	18.815015
49.199879	2038.948647	18.820032
49.064384	2043.053316	18.825050
49.350453	2050.444584	18.830067
49.513136	2049.973556	18.835085
49.527036	2045.812974	18.840103
49.557275	2045.078339	18.845120
49.682526	2049.861900	18.850138
49.774195	2041.816752	18.855155
49.257134	2046.967818	18.860173
49.849302	2040.234247	18.865191
49.724355	2038.158920	18.870208
49.615163	2042.843011	18.875226
49.832806	2038.739603	18.880243
49.509147	2052.264064	18.885261
49.914008	2041.398752	18.890279
49.916135	2057.527423	18.895296
49.967812	2062.292834	18.900314
50.427543	2062.637272	18.905331
50.249451	2061.442698	18.910349
50.588027	2054.220219	18.915367
50.596085	2052.784377	18.920384
50.404109	2048.122564	18.925402
50.565379	2038.766943	18.930419
50.648819	2029.712403	18.935437
50.700280	2026.227771	18.940455
50.615468	2030.729424	18.945472
50.657209	2022.367406	18.950490
50.495960	2032.410657	18.955507
50.247441	2036.229744	18.960525
50.300445	2021.829984	18.965543
50.464746	2042.188766	18.970560
50.699607	2049.982260	18.975578
50.878426	2052.020886	18.980595
50.647770	2053.278494	18.985613
50.968889	2059.028161	18.990631
50.822378	2055.317108	18.995648
50.874700	2049.302801	19.000666
50.956566	2048.759715	19.005683
50.617977	2048.144466	19.010701
50.988976	2045.707672	19.015719
51.074667	2043.045810	19.020736
50.983094	2049.212876	19.025754
50.892267	2051.800256	19.030771
50.889789	2072.455465	19.035789
51.108556	2080.129627	19.040807
51.194251	2086.037979	19.045824
51.358432	2086.976991	19.050842
51.303168	2076.112674	19.055859
50.817236	2083.100881	19.060877
51.332418	2091.326338	19.065895
51.339871	2093.258587	19.070912
51.880063	2101.576807	19.075930
51.787164	2110.977613	19.080947
52.040807	2112.371929	19.085965
52.036231	2106.800847	19.090983
52.120676	2108.477776	19.096000
51.956476	2118.087381	19.101018
52.455495	2105.475810	19.106035
52.057694	2105.124844	19.111053
52.085221	2107.274127	19.116071
52.088956	2102.588163	19.121088
52.197798	2101.607384	19.126106
52.239840	2106.267375	19.131123
51.979709	2110.522508	19.136141
52.511167	2103.896123	19.141159
52.067618	2100.571434	19.146176
52.331784	2097.049716	19.151194
52.623538	2095.838410	19.156211
52.319968	2108.321474	19.161229
52.232353	2109.715157	19.166247
52.249216	2112.092668	19.171264
52.542289	2124.810942	19.176282
52.711790	2136.071007	19.181299
52.846278	2137.891762	19.186317
53.071357	2129.881920	19.191335
53.156186	2127.302767	19.196352
52.840191	2132.878780	19.201370
53.295522	2132.553782	19.206387
53.132936	2133.590532	19.211405
53.271110	2123.701326	19.216423
52.989981	2126.684815	19.221440
52.760366	2121.457945	19.226458
52.633059	2121.728474	19.231475
53.270487	2129.759057	19.236493
53.090326	2119.440828	19.241511
52.954175	2129.435310	19.246528
53.167138	2143.458679	19.251546
53.406715	2151.466204	19.256563
53.263550	2161.059898	19.261581
53.699621	2162.963127	19.266599
53.553544	2156.139593	19.271616
53.700568	2149.994518	19.276634
53.680347	2146.072955	19.281651
53.684602	2157.751093	19.286669
53.804224	2146.565448	19.291687
53.643890	2153.991782	19.296704
53.629916	2147.955758	19.301722
53.953358	2148.971627	19.306739
53.665425	2151.236511	19.311757
54.048516	2156.221244	19.316775
54.188033	2177.381732	19.321792
54.335260	2181.958115	19.326810
54.181136	2166.496364	19.331827
54.098452	2173.894593	19.336845
54.458889	2178.900251	19.341863
54.529694	2182.865873	19.346880
54.811083	2182.663001	19.351898
54.817793	2173.468805	19.356915
54.197337	2171.063477	19.361933
54.422754	2173.571339	19.366951
54.653742	2178.666859	19.371968
54.615475	2175.131217	19.376986
54.672408	2176.835351	19.382003
54.374374	2188.274632	19.387021
54.832727	2176.028155	19.392039
54.669346	2170.914193	19.397056
54.478384	2176.958731	19.402074
54.861890	2169.066754	19.407091
54.818320	2182.140804	19.412109
55.123241	2200.197164	19.417127
54.962379	2208.421176	19.422144
54.965480	2208.369657	19.427162
54.944733	2206.469607	19.432179
54.953323	2211.580157	19.437197
55.169212	2201.572320	19.442215
55.329816	2205.486658	19.447232
55.274817	2212.598119	19.452250
55.529010	2210.718717	19.457267
55.345424	2234.992088	19.462285
55.537808	2245.893852	19.467303
55.699591	2239.446708	19.472320
55.582289	2238.030839	19.477338
55.823058	2238.113673	19.482355
55.624175	2243.903871	19.487373
55.787378	2232.854363	19.492391
55.855121	2231.659895	19.497408
55.992871	2234.669415	19.502426
56.280141	2239.038641	19.507443
56.185521	2243.692155	19.512461
56.098359	2237.044815	19.517479
56.360045	2238.518089	19.522496
56.104577	2236.919752	19.527514
56.374217	2231.242752	19.532531
56.351657	2236.989883	19.537549
56.488963	2239.448885	19.542567
56.596592	2247.663134	19.547584
56.114445	2242.758082	19.552602
56.504170	2238.929213	19.557619
56.554891	2246.372273	19.562637
56.336447	2251.165094	19.567655
56.843704	2262.855910	19.572672
56.741714	2265.196556	19.577690
57.074483	2265.570688	19.582707
56.571062	2265.941317	19.587725
56.774031	2268.159390	19.592743
56.888041	2261.804803	19.597760
56.511122	2272.680184	19.602778
56.904723	2255.627874	19.607795
56.981331	2263.057376	19.612813
56.640724	2267.926317	19.617831
56.991912	2282.054412	19.622848
56.940834	2286.899208	19.627866
57.299254	2291.296431	19.632883
57.299533	2300.422934	19.637901
57.206296	2293.176392	19.642919
57.125331	2300.419459	19.647936
57.267690	2305.024973	19.652954
58.086287	2309.385780	19.657971
57.890057	2307.475948	19.662989
57.767968	2296.156481	19.668007
57.636966	2295.891168	19.673024
57.738099	2317.625877	19.678042
57.884702	2324.380390	19.683059
57.781575	2329.666897	19.688077
57.871241	2312.411293	19.693095
58.359106	2304.480577	19.698112
58.450878	2314.666152	19.703130
58.259893	2308.484462	19.708147
58.285405	2316.139230	19.713165
58.544739	2313.830321	19.718183
58.697805	2313.244408	19.723200
58.553366	2312.506942	19.728218
58.590564	2308.581684	19.733235
58.645472	2303.554779	19.738253
58.809060	2309.082690	19.743271
59.128675	2312.240984	19.748288
58.639466	2293.516401	19.753306
58.875371	2283.821513	19.758323
58.675534	2284.924778	19.763341
58.735958	2300.946889	19.768359
59.127347	2298.284993	19.773376
58.628359	2302.954249	19.778394
59.011659	2310.095749	19.783411
58.742579	2307.058597	19.788429
58.843990	2316.119428	19.793447
59.067969	2307.341196	19.798464
58.821101	2307.408199	19.803482
58.640434	2318.674697	19.808499
59.300098	2334.720835	19.813517
59.312339	2349.004516	19.818535
59.397246	2342.637231	19.823552
59.463758	2355.563311	19.828570
59.716599	2341.040125	19.833587
59.714917	2339.660867	19.838605
59.551433	2349.397147	19.843623
59.463531	2346.318506	19.848640
59.609746	2348.761948	19.853658
59.596802	2341.164355	19.858675
59.720699	2346.789852	19.863693
59.227068	2343.338590	19.868711
59.646860	2360.134062	19.873728
59.560255	2369.794383	19.878746
59.949697	2370.085543	19.883763
59.939390	2371.969535	19.888781
59.804057	2375.813132	19.893799
60.142306	2378.925994	19.898816
60.281181	2385.139040	19.903834
60.511093	2399.233103	19.908851
60.633645	2398.320910	19.913869
60.401153	2393.756688	19.918887
60.785107	2388.888076	19.923904
60.580015	2391.821736	19.928922
60.614268	2391.133638	19.933939
60.593142	2393.481071	19.938957
60.611805	2394.359149	19.943975
60.927892	2380.815335	19.948992
60.896002	2393.344982	19.954010
60.699946	2393.614681	19.959027
61.127912	2377.202518	19.964045
60.855936	2398.152082	19.969063
60.947761	2389.881760	19.974080
61.109550	2395.687648	19.979098
61.234828	2415.153347	19.984115
61.512910	2418.757192	19.989133
61.376767	2417.699052	19.994151
61.576792	2418.262684	19.999168
61.673761	2414.452143	20.004186
61.329560	2422.297285	20.009203
61.389243	2421.065546	20.014221
61.599662	2415.684230	20.019239
61.621202	2409.751767	20.024256
61.555713	2421.725190	20.029274
61.586707	2416.173487	20.034291
61.563595	2425.206265	20.039309
61.708473	2448.058982	20.044327
62.123204	2452.930227	20.049344
62.288210	2446.513940	20.054362
62.267501	2450.679073	20.059379
62.436251	2447.166983	20.064397
62.173595	2445.414027	20.069415
62.389302	2444.274602	20.074432
62.412443	2450.622545	20.079450
62.846075	2441.562241	20.084467
62.897511	2439.349394	20.089485
62.514543	2453.236851	20.094503
62.661447	2442.387999	20.099520
62.634387	2440.246662	20.104538
62.400932	2440.812569	20.109555
62.368637	2442.927394	20.114573
62.429193	2441.599553	20.119591
62.659291	2429.685016	20.124608
62.652477	2434.855520	20.129626
62.710111	2453.882928	20.134643
62.873308	2457.560951	20.139661
63.040815	2466.960572	20.144679
63.374395	2464.906445	20.149696
63.310572	2457.198920	20.154714
63.276242	2467.298526	20.159731
63.432438	2465.654961	20.164749
63.374925	2464.316844	20.169767
63.370625	2466.903082	20.174784
63.381291	2460.291164	20.179802
63.255928	2453.925115	20.184819
63.539180	2463.181210	20.189837
63.381088	2484.347919	20.194855
63.576259	2480.017508	20.199872
63.785242	2487.845255	20.204890
63.741672	2480.084148	20.209907
63.984290	2490.866392	20.214925
63.948910	2479.274959	20.219943
63.935451	2490.837417	20.224960
64.031968	2495.065671	20.229978
64.313493	2484.885140	20.234995
64.493206	2483.146580	20.240013
64.047977	2499.460351	20.245031
64.378532	2500.767716	20.250048
64.418892	2503.082551	20.255066
64.459117	2517.855115	20.260083
64.394710	2515.932884	20.265101
64.372206	2524.044551	20.270119
64.326284	2511.270197	20.275136
64.350596	2523.196345	20.280154
64.311392	2527.201629	20.285171
65.023238	2521.820538	20.290189
65.056786	2547.936560	20.295207
64.995713	2540.963211	20.300224
65.115770	2525.455779	20.305242
65.297255	2550.443080	20.310259
65.388628	2530.608561	20.315277
65.366836	2537.640159	20.320295
65.598751	2532.784736	20.325312
65.658776	2528.585984	20.330330
65.445548	2527.905098	20.335347
65.746320	2521.651972	20.340365
65.216310	2548.778159	20.345383
65.403190	2538.633923	20.350400
65.789150	2534.423305	20.355418
65.268531	2535.067261	20.360435
65.528951	2538.486749	20.365453
65.965586	2553.076570	20.370471
65.803394	2551.041718	20.375488
66.327046	2555.102762	20.380506
66.206711	2559.495402	20.385523
66.149680	2552.522190	20.390541
66.219986	2559.706651	20.395559
66.229863	2553.065714	20.400576
66.298609	2550.360054	20.405594
66.293732	2552.594802	20.410611
66.622096	2549.878415	20.415629
66.505798	2555.505329	20.420647
66.603801	2559.936301	20.425664
66.809520	2545.757867	20.430682
66.732804	2552.681032	20.435699
66.844160	2543.008196	20.440717
66.632179	2547.786710	20.445735
66.803342	2539.402183	20.450752
66.720573	2544.468426	20.455770
66.676118	2550.300976	20.460787
67.103525	2545.793499	20.465805
67.166745	2544.108120	20.470823
67.203107	2551.256302	20.475840
67.092829	2552.663079	20.480858
66.873176	2567.840536	20.485875
67.294338	2582.598822	20.490893
67.167351	2584.812933	20.495911
66.976043	2575.424316	20.500928
67.216711	2575.691228	20.505946
67.364383	2596.771581	20.510963
67.637534	2604.191150	20.515981
67.548207	2604.487879	20.520999
67.851432	2604.328717	20.526016
68.199961	2607.826986	20.531034
67.578974	2612.256223	20.536051
68.076092	2607.515010	20.541069
68.293010	2603.330545	20.546087
68.012537	2600.369871	20.551104
68.333489	2594.185860	20.556122
68.203184	2610.003542	20.561139
68.328199	2604.145741	20.566157
68.571411	2615.266211	20.571175
68.895884	2625.805035	20.576192
68.584004	2610.383701	20.581210
68.557027	2620.370547	20.586227
69.020496	2612.699194	20.591245
69.084653	2625.525995	20.596263
68.809782	2615.301175	20.601280
69.094850	2604.669288	20.606298
68.798579	2624.417229	20.611315
68.760050	2616.368145	20.616333
68.983428	2629.356761	20.621351
69.136083	2625.736289	20.626368
69.511610	2623.870522	20.631386
69.170645	2629.232036	20.636403
69.061296	2616.975046	20.641421
69.369662	2617.609506	20.646439
68.898172	2629.571549	20.651456
69.760961	2616.103153	20.656474
69.435627	2619.837103	20.661491
69.648170	2633.315129	20.666509
69.802066	2648.647046	20.671527
69.572674	2639.359637	20.676544
69.743099	2648.028178	20.681562
70.014629	2650.559448	20.686579
69.744787	2644.965179	20.691597
69.922078	2645.681110	20.696615
70.068364	2652.936878	20.701632
70.245064	2650.874709	20.706650
70.075148	2649.504946	20.711667
70.335380	2640.970079	20.716685
70.245081	2650.089222	20.721703
70.459068	2647.900761	20.726720
70.555643	2652.048820	20.731738
70.631400	2665.682408	20.736755
70.676264	2674.655732	20.741773
70.757583	2671.284171	20.746791
70.675691	2679.919819	20.751808
70.734677	2674.848088	20.756826
70.917759	2664.343330	20.761843
71.071437	2664.075871	20.766861
70.709161	2673.535730	20.771879
70.879296	2675.295022	20.776896
71.506220	2673.643223	20.781914
71.024242	2680.653103	20.786931
70.895854	2683.758647	20.791949
71.448186	2695.865021	20.796967
71.438721	2706.277032	20.801984
71.508531	2698.286136	20.807002
71.332632	2707.205803	20.812019
71.545137	2692.559702	20.817037
71.498291	2711.816486	20.822055
71.317211	2711.429365	20.827072
72.099714	2717.919042	20.832090
71.955588	2728.938548	20.837107
71.914422	2732.236277	20.842125
72.078081	2741.359025	20.847143
72.108030	2741.068822	20.852160
72.476550	2722.874705	20.857178
72.213926	2728.393662	20.862195
72.443665	2723.175122	20.867213
72.180112	2730.102210	20.872231
72.222230	2722.405180	20.877248
72.681045	2719.354899	20.882266
72.346874	2743.820672	20.887283
72.680412	2752.895099	20.892301
72.643844	2759.029308	20.897319
72.877523	2756.422374	20.902336
72.964597	2754.136936	20.907354
72.900535	2749.235039	20.912371
73.420346	2735.875506	20.917389
73.548495	2749.783988	20.922407
73.292090	2749.554396	20.927424
73.840753	2740.274987	20.932442
73.664525	2738.658448	20.937459
73.737605	2747.772835	20.942477
73.977496	2736.981301	20.947495
73.747783	2734.297247	20.952512
73.622152	2714.840821	20.957530
73.381638	2728.521760	20.962547
73.266713	2740.637833	20.967565
73.419783	2733.944875	20.972583
73.320946	2743.742685	20.977600
73.887357	2733.307319	20.982618
73.715316	2746.179760	20.987635
73.668626	2763.973543	20.992653
74.488620	2763.923895	20.997671
74.123709	2766.333292	21.002688
74.397673	2763.963774	21.007706
74.199697	2772.014678	21.012723
74.444975	2768.992149	21.017741
74.461150	2771.191322	21.022759
74.219104	2765.134781	21.027776
74.516593	2768.787535	21.032794
74.628743	2787.332375	21.037811
74.614661	2793.709214	21.042829
74.954131	2793.804631	21.047847
74.876131	2796.539546	21.052864
75.041035	2782.947893	21.057882
74.864813	2793.574554	21.062899
74.960749	2792.568258	21.067917
75.176878	2781.019067	21.072935
74.914785	2793.078421	21.077952
75.225534	2812.181560	21.082970
75.433013	2827.219589	21.087987
75.638011	2812.928530	21.093005
75.820873	2818.696618	21.098023
75.717025	2827.506544	21.103040
75.834159	2823.794937	21.108058
76.070708	2810.719632	21.113075
75.948898	2811.204819	21.118093
76.158092	2823.646048	21.123111
75.820356	2833.891829	21.128128
76.388961	2801.767487	21.133146
76.166916	2818.094787	21.138163
76.466741	2820.666410	21.143181
76.255423	2808.486088	21.148199
75.930848	2809.821662	21.153216
76.348612	2817.519542	21.158234
76.558431	2825.337113	21.163251
76.677955	2832.712081	21.168269
76.563026	2842.378017	21.173287
76.155064	2835.253761	21.178304
76.588857	2828.468796	21.183322
76.830655	2845.432444	21.188339
76.784943	2869.097299	21.193357
76.583590	2868.777906	21.198375
77.257582	2864.480360	21.203392
77.117141	2865.007849	21.208410
77.341024	2869.901021	21.213427
76.907246	2858.994226	21.218445
77.551878	2847.714093	21.223463
77.424288	2864.307980	21.228480
77.554222	2860.812995	21.233498
77.584287	2867.701975	21.238515
77.551213	2889.374775	21.243533
77.866280	2878.661607	21.248551
77.936860	2884.214797	21.253568
78.026715	2883.848963	21.258586
77.883066	2886.782360	21.263603
77.965573	2890.197269	21.268621
78.357871	2875.213970	21.273639
78.293570	2887.827869	21.278656
78.101580	2883.121738	21.283674
77.981980	2885.158519	21.288691
77.904787	2886.667028	21.293709
78.190523	2902.013583	21.298727
78.410121	2903.599045	21.303744
78.812290	2910.426345	21.308762
79.054544	2909.549307	21.313779
78.658848	2910.787681	21.318797
79.164648	2899.083652	21.323815
78.933767	2911.635253	21.328832
79.266816	2905.545148	21.333850
79.322275	2905.822725	21.338867
79.238468	2911.225136	21.343885
79.108958	2909.891379	21.348903
79.105013	2919.292678	21.353920
79.477214	2944.569598	21.358938
79.526162	2938.780429	21.363955
79.633558	2943.701641	21.368973
80.115857	2933.296854	21.373991
79.703529	2936.445371	21.379008
80.334388	2926.445591	21.384026
80.324708	2927.378563	21.389043
80.227107	2936.521074	21.394061
80.673464	2914.397857	21.399079
80.321964	2929.551092	21.404096
80.425303	2922.236703	21.409114
80.233328	2924.856885	21.414131
80.074628	2922.406887	21.419149
80.318870	2920.971051	21.424167
80.099390	2933.402076	21.429184
80.247557	2936.599650	21.434202
80.407445	2945.324326	21.439219
80.495838	2953.303704	21.444237
80.809583	2949.505649	21.449255
80.717235	2962.943718	21.454272
80.703563	2957.669522	21.459290
80.905057	2960.955348	21.464307
81.054556	2984.195962	21.469325
81.266192	2977.017662	21.474343
81.344491	2979.457097	21.479360
81.549638	2983.336227	21.484378
81.674041	2973.521798	21.489395
81.820177	2989.604150	21.494413
82.082238	2983.235080	21.499431
81.919023	2976.590877	21.504448
82.142612	2962.333677	21.509466
81.759340	2950.862635	21.514483
81.476202	2954.345308	21.519501
82.097163	2966.709195	21.524519
82.171964	2979.351333	21.529536
81.684966	2977.975468	21.534554
81.783521	2973.009807	21.539571
81.863637	2975.146899	21.544589
82.268264	2994.200697	21.549607
82.576910	3007.938267	21.554624
82.509019	3001.477860	21.559642
82.881015	3002.568644	21.564659
82.818346	3007.804107	21.569677
82.885816	2997.239675	21.574695
82.958404	3016.912803	21.579712
83.053146	3003.019068	21.584730
83.250245	2999.487381	21.589747
83.028741	3000.272434	21.594765
83.110536	3002.318804	21.599783
83.152488	3002.229624	21.604800
83.245754	3002.827612	21.609818
83.363096	2998.812301	21.614835
83.170403	3007.417043	21.619853
83.744432	3018.592831	21.624871
83.555976	3022.002212	21.629888
83.666319	3033.493442	21.634906
84.141933	3022.208668	21.639923
83.558734	3034.221102	21.644941
83.690513	3025.489396	21.649959
83.896651	3025.422015	21.654976
84.061660	3033.746334	21.659994
84.078087	3045.371327	21.665011
83.888625	3057.656869	21.670029
84.121602	3057.368893	21.675047
84.189213	3049.041492	21.680064
84.199234	3058.116573	21.685082
84.510144	3068.432129	21.690099
84.688601	3083.346049	21.695117
84.592523	3075.470288	21.700135
84.601175	3092.745928	21.705152
84.965381	3093.394319	21.710170
84.967120	3077.025750	21.715187
85.221188	3079.098933	21.720205
85.783315	3096.067639	21.725223
85.681584	3089.402567	21.730240
85.272652	3099.635502	21.735258
85.365731	3090.714850	21.740275
85.289875	3106.123218	21.745293
85.701654	3113.130788	21.750311
85.761215	3103.522476	21.755328
85.582397	3115.609719	21.760346
86.150214	3106.801349	21.765363
85.819024	3111.993144	21.770381
86.237422	3105.297034	21.775399
86.158379	3114.505131	21.780416
85.877239	3103.916768	21.785434
86.212883	3106.175957	21.790451
86.065750	3103.346515	21.795469
86.220246	3119.024937	21.800487
86.476787	3127.160087	21.805504
86.573546	3124.921030	21.810522
86.690985	3128.116468	21.815539
86.625686	3136.107870	21.820557
86.858845	3125.745824	21.825575
86.892625	3130.688279	21.830592
86.800781	3123.747876	21.835610
86.926748	3127.502802	21.840627
86.974875	3146.249453	21.845645
87.177470	3149.106448	21.850663
87.432472	3159.577293	21.855680
87.234446	3156.642685	21.860698
87.542575	3146.671411	21.865715
87.346030	3151.298990	21.870733
87.789654	3141.931464	21.875751
87.908573	3146.562223	21.880768
87.910588	3149.383557	21.885786
88.174454	3151.327758	21.890803
88.243055	3162.340411	21.895821
88.342271	3161.281652	21.900839
88.429946	3176.484670	21.905856
88.207367	3177.659273	21.910874
88.998582	3168.651628	21.915891
88.735179	3174.076482	21.920909
88.568506	3164.080227	21.925927
88.999478	3164.083184	21.930944
88.742068	3173.909716	21.935962
89.102189	3167.282655	21.940979
89.050529	3161.960953	21.945997
89.187209	3165.420777	21.951015
89.128825	3167.835631	21.956032
88.846896	3159.659088	21.961050
89.443337	3158.977268	21.966067
89.098580	3162.652308	21.971085
89.160836	3159.991621	21.976103
89.438903	3160.033120	21.981120
89.109424	3162.620995	21.986138
89.691016	3173.407901	21.991155
89.727774	3187.321149	21.996173
89.879780	3184.719300	22.001191
89.964193	3191.384236	22.006208
89.479567	3201.078687	22.011226
89.930712	3187.679353	22.016243
89.985467	3203.739545	22.021261
90.125818	3201.638260	22.026279
90.221679	3209.342848	22.031296
90.436182	3218.677253	22.036314
90.352526	3209.132614	22.041331
90.193523	3208.347080	22.046349
90.487743	3212.106661	22.051367
90.581761	3207.896788	22.056384
90.804889	3231.127627	22.061402
91.204194	3233.775496	22.066419
91.586279	3238.002478	22.071437
91.406023	3233.873306	22.076455
91.271147	3224.718331	22.081472
91.052100	3235.242015	22.086490
91.553943	3233.281306	22.091507
91.299613	3238.432569	22.096525
91.265320	3227.631697	22.101543
91.709503	3222.340241	22.106560
91.725261	3233.753892	22.111578
91.997631	3227.728395	22.116595
91.573290	3223.283389	22.121613
91.962175	3241.723321	22.126631
92.177731	3255.595536	22.131648
92.252249	3255.193596	22.136666
92.408427	3248.726452	22.141683
92.270155	3254.520753	22.146701
92.248325	3253.025843	22.151719
92.495318	3241.328205	22.156736
92.116495	3262.288963	22.161754
92.618448	3267.521006	22.166771
92.531113	3280.707638	22.171789
92.621597	3284.304648	22.176807
92.931100	3288.204976	22.181824
92.702712	3290.815296	22.186842
92.889331	3288.476930	22.191859
93.046239	3311.545402	22.196877
93.192897	3313.375380	22.201895
93.635753	3310.103342	22.206912
93.232963	3315.895799	22.211930
93.509357	3308.680267	22.216947
93.509619	3317.834941	22.221965
93.594528	3326.204453	22.226983
94.205427	3331.839199	22.232000
94.273692	3336.010847	22.237018
94.230034	3338.172451	22.242035
94.082893	3331.663965	22.247053
94.269452	3335.546941	22.252071
94.344807	3330.202563	22.257088
94.283514	3328.443343	22.262106
94.457908	3323.795061	22.267123
94.510899	3335.176109	22.272141
94.623580	3356.621052	22.277159
95.339795	3350.999056	22.282176
95.257780	3363.476959	22.287194
95.557700	3354.940070	22.292211
95.269739	3349.752736	22.297229
95.325502	3354.483307	22.302247
95.681965	3342.396063	22.307264
95.202361	3332.190798	22.312282
95.430709	3336.495815	22.317299
95.750973	3341.258932	22.322317
95.831252	3355.421050	22.327335
95.887270	3348.734636	22.332352
95.778003	3348.572028	22.337370
95.801359	3347.248464	22.342387
95.919054	3347.616813	22.347405
96.093032	3344.828150	22.352423
96.195877	3345.634653	22.357440
96.033396	3352.559287	22.362458
95.967707	3346.427180	22.367475
96.224980	3354.709440	22.372493
96.087624	3373.817914	22.377511
96.313224	3376.159985	22.382528
96.468380	3376.151077	22.387546
96.427455	3377.846573	22.392563
96.693261	3394.036935	22.397581
96.860709	3402.370517	22.402599
97.147870	3396.011426	22.407616
96.986640	3404.716002	22.412634
97.132788	3399.970727	22.417651
97.060068	3410.619873	22.422669
97.400520	3432.602838	22.427687
97.690140	3426.197718	22.432704
97.847582	3426.405553	22.437722
98.215735	3426.032300	22.442739
97.672288	3425.521232	22.447757
97.730416	3431.573760	22.452775
98.415113	3424.704463	22.457792
98.027242	3432.382474	22.462810
97.991419	3428.798941	22.467827
98.678148	3445.818984	22.472845
98.632247	3448.924907	22.477863
98.630807	3456.981816	22.482880
98.593886	3457.512483	22.487898
98.785705	3444.857510	22.492915
98.793471	3454.899955	22.497933
98.576928	3451.804622	22.502951
98.958897	3441.532684	22.507968
98.654364	3460.217196	22.512986
98.995123	3464.582988	22.518003
99.625307	3475.356079	22.523021
99.568461	3481.562261	22.528039
99.767126	3476.921860	22.533056
99.850384	3473.090419	22.538074
99.751396	3473.282510	22.543091
99.965623	3464.675840	22.548109
99.623831	3473.620852	22.553127
99.888220	3460.100809	22.558144
100.067506	3468.887995	22.563162
100.027010	3476.062259	22.568179
99.960037	3486.580752	22.573197
100.191769	3496.801472	22.578215
100.127363	3496.076352	22.583232
100.416533	3505.071012	22.588250
100.450265	3499.059860	22.593267
100.434635	3510.230946	22.598285
100.613181	3527.494954	22.603303
100.856111	3528.106070	22.608320
100.718425	3532.998914	22.613338
100.822752	3537.694269	22.618355
101.417034	3521.981940	22.623373
101.009797	3524.668804	22.628391
101.474815	3549.144563	22.633408
101.596036	3555.210680	22.638426
101.699189	3544.525316	22.643443
101.885848	3543.371563	22.648461
101.588072	3548.131829	22.653479
101.898345	3541.090132	22.658496
101.854876	3550.316429	22.663514
101.908078	3552.803227	22.668531
102.013444	3564.504912	22.673549
102.347882	3571.106553	22.678567
102.450806	3566.898304	22.683584
102.546834	3579.266977	22.688602
102.632451	3576.766895	22.693619
102.639066	3567.716575	22.698637
102.763869	3576.936507	22.703655
103.268745	3574.126501	22.708672
102.860889	3564.260466	22.713690
103.108292	3572.808731	22.718707
103.476764	3575.651946	22.723725
103.508169	3584.200050	22.728743
103.288254	3575.169330	22.733760
103.440084	3591.245146	22.738778
103.808746	3580.318399	22.743795
103.858452	3573.394541	22.748813
103.698133	3591.737638	22.753831
103.830771	3585.410187	22.758848
104.031510	3582.540123	22.763866
104.194492	3608.685387	22.768883
104.317986	3603.956245	22.773901
104.178689	3608.833639	22.778919
104.417179	3606.375251	22.783936
104.516600	3613.605934	22.788954
104.314162	3618.542957	22.793971
104.698722	3605.595950	22.798989
104.566633	3613.035035	22.804007
105.048596	3631.468487	22.809024
105.038051	3637.386524	22.814042
105.020367	3639.411876	22.819059
105.370766	3643.905193	22.824077
104.930094	3645.752567	22.829095
105.065171	3643.085687	22.834112
105.320209	3669.490128	22.839130
105.698057	3661.815372	22.844147
105.646308	3666.423168	22.849165
105.657758	3674.562311	22.854183
106.095122	3666.193691	22.859200
105.983442	3665.996851	22.864218
105.932123	3676.081908	22.869235
106.267110	3673.287175	22.874253
106.168702	3682.399600	22.879271
106.393165	3690.168892	22.884288
106.431956	3691.203526	22.889306
106.427493	3692.809074	22.894323
106.442428	3690.765478	22.899341
106.559923	3693.902822	22.904359
106.981161	3707.519265	22.909376
107.256668	3716.399812	22.914394
107.069242	3728.003577	22.919411
107.556901	3720.660545	22.924429
107.462241	3715.513052	22.929447
107.638807	3721.084272	22.934464
108.010855	3716.076322	22.939482
107.907839	3705.201885	22.944499
108.169491	3709.337297	22.949517
107.959711	3713.131754	22.954535
108.128629	3708.226995	22.959552
108.468929	3705.971828	22.964570
108.118528	3710.767283	22.969587
108.209497	3695.260104	22.974605
108.150217	3711.277680	22.979623
108.495229	3725.172965	22.984640
108.299395	3728.674934	22.989658
108.649717	3740.653927	22.994675
108.698395	3729.160585	22.999693
109.021991	3736.281639	23.004711
109.040755	3746.823618	23.009728
109.309359	3740.428007	23.014746
109.204767	3757.681586	23.019763
109.451289	3761.453638	23.024781
109.563726	3764.904886	23.029799
109.843310	3757.810555	23.034816
109.824450	3755.487577	23.039834
109.798607	3751.487028	23.044851
110.154168	3742.050570	23.049869
109.883298	3745.240414	23.054887
109.748616	3754.148635	23.059904
110.326966	3766.312333	23.064922
110.509808	3781.993242	23.069939
110.568856	3776.854256	23.074957
110.829948	3778.168890	23.079975
110.535667	3765.343364	23.084992
110.510618	3769.945362	23.090010
110.379583	3786.811446	23.095027
111.039793	3793.852892	23.100045
111.050104	3806.170921	23.105063
110.961518	3799.169891	23.110080
111.196486	3787.358101	23.115098
111.376087	3796.918703	23.120115
111.703315	3802.223644	23.125133
111.643430	3820.381097	23.130151
112.120220	3822.178164	23.135168
111.747253	3817.019162	23.140186
111.659999	3821.484780	23.145203
112.265150	3815.119642	23.150221
112.003601	3827.470814	23.155239
112.063286	3828.720812	23.160256
112.657360	3818.303875	23.165274
112.553228	3822.597551	23.170291
112.418944	3822.316995	23.175309
112.458944	3842.363007	23.180327
113.051377	3838.111236	23.185344
113.248052	3836.515345	23.190362
113.059741	3846.996806	23.195379
113.444473	3844.858823	23.200397
113.557247	3840.449904	23.205415
113.536749	3840.608244	23.210432
113.598380	3831.556855	23.215450
113.510578	3841.752466	23.220467
113.834038	3846.645825	23.225485
113.799707	3845.697991	23.230503
113.752181	3845.129849	23.235520
114.146863	3858.566595	23.240538
114.072669	3870.209054	23.245555
114.452589	3865.560081	23.250573
114.503668	3870.046134	23.255591
114.347097	3876.562590	23.260608
114.606051	3867.643336	23.265626
114.684222	3865.405558	23.270643
114.428322	3861.834986	23.275661
114.585497	3898.025561	23.280679
114.753788	3901.438828	23.285696
115.167124	3895.198641	23.290714
115.072622	3893.479260	23.295731
115.470444	3911.971323	23.300749
115.402569	3921.393686	23.305767
115.407430	3935.839786	23.310784
115.559168	3928.786213	23.315802
115.434244	3924.127260	23.320819
115.761894	3934.937138	23.325837
115.705756	3952.318523	23.330855
115.920250	3954.378480	23.335872
116.355598	3954.018103	23.340890
116.059669	3962.059317	23.345907
116.582366	3962.971968	23.350925
116.890653	3971.251952	23.355943
116.752597	3986.487874	23.360960
116.820023	3968.658824	23.365978
116.873062	3967.723796	23.370995
117.106529	3954.522890	23.376013
117.231374	3952.667834	23.381031
117.349920	3966.487757	23.386048
117.764590	3963.139837	23.391066
117.599400	3982.711372	23.396083
117.847289	3984.436402	23.401101
118.212419	3978.922865	23.406119
117.754650	3990.671422	23.411136
118.403743	3982.742426	23.416154
118.122768	3979.149863	23.421171
117.917251	3988.720081	23.426189
118.123987	3987.828982	23.431207
118.147884	3985.692666	23.436224
118.361763	3989.915228	23.441242
118.254103	4000.774903	23.446259
118.532252	4008.140906	23.451277
119.056426	4011.735020	23.456295
118.613671	4008.086435	23.461312
119.057668	4015.475555	23.466330
119.169153	4019.154357	23.471347
119.234592	4030.080850	23.476365
119.268356	4042.416577	23.481383
119.310694	4042.985759	23.486400
119.966306	4037.450267	23.491418
119.329354	4031.368845	23.496435
119.734155	4057.695829	23.501453
120.346102	4055.800062	23.506471
120.384145	4062.879491	23.511488
120.805707	4056.460141	23.516506
120.761568	4058.109815	23.521523
120.849273	4053.690671	23.526541
121.150616	4061.473862	23.531559
120.680091	4060.661647	23.536576
120.618938	4046.411041	23.541594
120.703309	4056.848383	23.546611
121.015012	4067.324216	23.551629
121.311598	4052.894629	23.556647
121.122685	4090.013264	23.561664
121.278253	4086.972522	23.566682
121.763789	4076.796910	23.571699
121.575720	4081.989031	23.576717
121.824150	4082.907666	23.581735
121.854437	4101.737839	23.586752
122.225895	4109.944111	23.591770
122.318980	4112.085597	23.596787
122.310912	4109.344700	23.601805
122.711526	4094.219600	23.606823
122.558523	4107.574777	23.611840
122.853509	4098.025820	23.616858
122.449535	4095.669011	23.621875
122.886244	4120.250937	23.626893
123.316862	4123.414750	23.631911
123.262476	4132.009107	23.636928
123.497880	4126.923690	23.641946
123.454897	4140.306979	23.646963
123.246607	4135.676984	23.651981
123.756884	4129.706799	23.656999
123.606077	4136.055678	23.662016
123.626672	4148.731858	23.667034
124.020641	4151.034623	23.672051
123.834943	4155.081804	23.677069
124.160427	4150.818234	23.682087
123.830563	4162.436399	23.687104
124.264741	4173.696745	23.692122
124.556477	4193.596898	23.697139
124.278275	4189.462617	23.702157
124.732773	4182.197021	23.707175
124.924053	4186.350871	23.712192
124.644761	4198.576169	23.717210
124.634606	4207.579661	23.722227
125.043162	4213.531796	23.727245
125.004860	4211.240953	23.732263
124.870701	4226.688900	23.737280
125.439418	4232.711478	23.742298
125.451836	4239.387587	23.747315
125.294086	4264.834689	23.752333
125.771727	4265.417854	23.757351
125.701355	4276.164013	23.762368
126.168284	4263.556510	23.767386
126.439735	4284.776112	23.772403
126.595481	4286.378992	23.777421
126.745230	4288.486295	23.782439
126.760048	4290.301234	23.787456
127.134704	4285.103092	23.792474
127.292556	4283.515705	23.797491
126.924019	4292.421421	23.802509
127.212400	4291.669114	23.807527
127.260738	4310.123796	23.812544
127.708472	4311.895668	23.817562
127.764762	4309.719525	23.822579
127.710967	4317.416308	23.827597
127.659141	4312.321561	23.832615
127.803946	4320.696253	23.837632
128.281467	4333.733975	23.842650
128.211143	4340.728551	23.847667
127.983502	4345.791768	23.852685
128.496324	4339.671626	23.857703
128.548511	4351.068539	23.862720
128.660084	4352.176575	23.867738
128.737846	4354.247380	23.872755
129.205556	4360.087876	23.877773
129.490973	4362.609373	23.882791
129.118305	4371.633009	23.887808
129.515780	4357.617347	23.892826
129.816850	4370.749318	23.897843
129.663891	4390.155816	23.902861
129.979116	4389.198623	23.907879
130.104429	4390.331218	23.912896
130.236615	4383.501600	23.917914
130.234066	4390.789048	23.922931
130.359548	4392.891582	23.927949
130.679521	4379.837770	23.932967
130.488101	4385.183933	23.937984
130.792465	4398.233590	23.943002
131.046313	4411.810518	23.948019
130.834240	4415.345917	23.953037
130.822263	4403.816093	23.958055
131.325680	4408.285252	23.963072
131.317852	4399.050281	23.968090
131.129135	4411.332900	23.973107
131.405828	4413.592261	23.978125
131.372036	4419.176051	23.983143
131.292351	4436.673471	23.988160
131.648476	4441.181073	23.993178
131.783949	4441.635513	23.998195
131.632098	4474.070853	24.003213
131.941661	4471.891276	24.008231
131.787108	4474.094329	24.013248
132.570584	4489.471755	24.018266
132.935565	4500.184060	24.023283
132.534362	4502.161335	24.028301
133.116637	4490.144923	24.033319
132.804316	4497.218281	24.038336
132.890195	4518.870590	24.043354
133.331067	4510.227960	24.048371
133.418605	4530.593804	24.053389
133.752350	4522.431602	24.058407
134.081343	4526.374002	24.063424
133.935780	4510.046986	24.068442
134.332314	4529.355824	24.073459
134.600369	4542.261144	24.078477
134.382385	4530.222832	24.083495
134.670438	4545.931051	24.088512
134.457990	4547.573789	24.093530
135.193155	4542.996194	24.098547
134.908537	4539.964187	24.103565
134.907033	4545.667172	24.108583
135.039632	4546.802551	24.113600
135.304142	4544.237594	24.118618
135.148588	4535.690836	24.123635
135.353910	4567.633612	24.128653
135.795774	4555.047952	24.133671
135.578220	4563.198930	24.138688
135.842215	4565.095320	24.143706
136.289479	4560.268620	24.148723
136.055137	4573.010202	24.153741
136.169366	4582.364618	24.158759
136.414632	4590.570830	24.163776
136.667299	4596.145985	24.168794
136.882406	4586.293991	24.173811
136.859761	4597.056374	24.178829
136.834576	4581.016105	24.183847
136.787110	4601.186448	24.188864
136.734994	4613.688966	24.193882
137.108119	4619.435301	24.198899
137.213081	4624.440072	24.203917
137.283930	4645.575753	24.208935
137.869705	4646.679790	24.213952
138.004104	4646.317828	24.218970
138.186982	4644.840482	24.223987
137.453475	4654.956316	24.229005
137.959445	4662.952649	24.234023
138.187906	4674.556926	24.239040
138.624105	4670.569776	24.244058
138.825776	4665.141839	24.249075
138.700986	4674.956088	24.254093
138.804509	4689.500481	24.259111
139.378025	4689.570408	24.264128
139.372669	4701.110505	24.269146
139.378346	4699.611848	24.274163
139.309472	4701.947596	24.279181
139.182136	4698.454652	24.284199
139.535145	4705.265471	24.289216
139.552726	4717.609066	24.294234
140.142943	4727.936336	24.299251
140.280468	4730.197484	24.304269
140.693679	4725.494951	24.309287
140.714886	4711.499616	24.314304
140.605931	4710.807497	24.319322
141.119561	4703.539301	24.324339
140.868695	4718.008851	24.329357
141.475010	4732.155295	24.334375
141.409059	4738.643521	24.339392
140.890928	4743.639907	24.344410
141.643080	4736.674300	24.349427
141.680890	4734.307516	24.354445
141.740809	4743.808365	24.359463
141.954052	4742.923267	24.364480
142.062155	4746.852960	24.369498
142.249380	4748.608211	24.374515
141.753427	4756.780084	24.379533
142.305908	4754.410690	24.384551
142.225029	4760.220031	24.389568
142.304772	4776.467555	24.394586
142.882377	4785.079528	24.399603
142.886287	4791.162504	24.404621
143.248575	4785.155081	24.409639
143.116581	4793.618233	24.414656
143.407574	4807.355598	24.419674
143.788021	4810.621183	24.424691
143.705624	4807.693760	24.429709
143.640446	4799.522638	24.434727
143.868268	4802.302779	24.439744
143.829058	4808.734063	24.444762
144.227077	4820.935270	24.449779
144.313233	4822.562680	24.454797
144.847090	4839.844748	24.459815
144.589505	4841.189476	24.464832
145.095460	4835.764095	24.469850
145.243614	4828.059281	24.474867
144.939529	4841.001808	24.479885
145.021667	4842.588953	24.484903
145.718446	4855.798299	24.489920
145.140632	4855.559332	24.494938
145.761014	4861.910645	24.499955
145.494506	4858.378490	24.504973
145.708188	4882.587391	24.509991
145.935474	4891.089290	24.515008
146.110483	4892.969232	24.520026
146.637534	4875.207403	24.525043
146.155306	4894.438137	24.530061
146.578935	4889.917979	24.535079
146.938762	4903.594898	24.540096
146.450375	4902.728045	24.545114
146.736310	4910.651821	24.550131
147.125605	4905.430677	24.555149
147.249238	4931.204600	24.560167
146.955184	4936.299061	24.565184
146.983087	4939.135492	24.570202
147.733514	4950.777129	24.575219
147.451365	4964.807422	24.580237
147.862091	4967.582032	24.585255
148.200712	4969.252595	24.590272
148.281005	4967.506789	24.595290
148.375340	4988.627419	24.600307
148.673184	4992.001407	24.605325
148.735116	4993.553242	24.610343
149.021285	4999.904408	24.615360
148.725908	4998.414386	24.620378
149.398421	5005.505606	24.625395
149.341881	5024.704823	24.630413
149.374695	5025.005722	24.635431
149.736786	5030.360627	24.640448
149.692619	5022.230087	24.645466
149.850662	5032.656377	24.650483
150.126261	5040.312032	24.655501
150.360099	5038.899687	24.660519
150.295865	5040.326889	24.665536
150.350449	5051.786901	24.670554
150.658999	5054.887783	24.675571
150.793160	5078.204185	24.680589
150.878601	5071.112649	24.685607
151.326686	5072.477049	24.690624
151.232734	5073.562842	24.695642
151.404730	5081.244477	24.700659
151.560860	5099.479206	24.705677
151.756353	5096.083381	24.710695
151.994378	5096.914059	24.715712
151.610958	5104.965907	24.720730
152.200185	5109.519944	24.725747
152.617107	5129.905691	24.730765
152.466374	5134.866441	24.735783
152.720433	5133.476825	24.740800
152.722856	5125.872976	24.745818
152.973493	5124.763976	24.750835
153.181523	5153.877795	24.755853
153.344255	5146.171278	24.760871
153.851298	5153.863255	24.765888
153.502369	5161.148095	24.770906
153.756010	5161.620693	24.775923
153.803903	5152.565962	24.780941
153.868451	5167.323948	24.785959
154.421775	5171.112751	24.790976
153.996232	5175.533589	24.795994
154.379464	5179.532032	24.801011
154.341356	5178.159100	24.806029
154.431473	5172.570181	24.811047
154.632684	5188.720909	24.816064
154.374374	5208.301050	24.821082
154.840964	5206.170284	24.826099
155.090890	5215.954256	24.831117
154.987729	5232.215712	24.836135
155.291657	5228.847411	24.841152
155.140185	5250.864343	24.846170
155.747811	5260.673918	24.851187
155.896385	5264.613031	24.856205
156.151932	5259.752952	24.861223
156.932347	5273.863511	24.866240
156.788012	5277.706934	24.871258
156.630476	5280.704380	24.876275
156.758970	5281.962414	24.881293
156.757314	5282.990236	24.886311
157.476220	5278.713183	24.891328
157.441451	5285.768621	24.896346
157.748853	5296.766046	24.901363
157.713701	5304.401367	24.906381
157.842565	5310.004404	24.911399
157.922564	5300.129421	24.916416
157.620845	5311.895834	24.921434
158.368731	5322.577590	24.926451
158.774088	5327.407258	24.931469
158.514257	5329.659476	24.936487
158.796783	5319.490211	24.941504
158.838967	5330.123212	24.946522
159.187836	5332.253204	24.951539
159.345533	5334.638680	24.956557
159.299693	5363.372495	24.961575
159.832947	5342.423676	24.966592
159.568410	5359.160220	24.971610
159.714538	5349.644420	24.976627
159.859569	5371.222469	24.981645
159.929032	5390.801728	24.986663
160.284446	5375.660502	24.991680
160.423448	5385.527571	24.996698
160.405166	5384.769038	25.001715
160.467963	5409.543344	25.006733
161.006751	5401.063963	25.011751
161.371613	5403.495879	25.016768
161.366991	5410.244468	25.021786
161.455072	5421.236831	25.026803
161.778681	5422.408698	25.031821
161.560885	5435.765178	25.036839
162.102391	5431.757107	25.041856
161.981358	5427.263838	25.046874
162.224049	5425.957829	25.051891
162.350162	5440.641761	25.056909
162.280440	5454.055682	25.061927
162.702196	5454.905079	25.066944
162.451645	5452.894127	25.071962
162.608687	5462.410638	25.076979
163.262316	5476.149817	25.081997
162.915519	5491.205010	25.087015
163.780156	5489.362411	25.092032
163.456469	5471.851161	25.097050
163.521312	5489.849962	25.102067
163.669367	5504.400648	25.107085
163.552903	5505.244601	25.112103
164.094302	5505.091511	25.117120
164.279068	5521.656688	25.122138
164.485237	5525.414395	25.127155
164.874251	5551.357150	25.132173
164.625200	5544.615317	25.137191
164.761701	5549.694049	25.142208
164.776607	5569.777887	25.147226
164.815554	5574.281344	25.152243
165.467366	5584.659983	25.157261
165.822375	5600.813392	25.162279
166.047109	5593.616004	25.167296
165.632452	5591.296835	25.172314
165.768903	5607.489817	25.177331
166.397407	5618.854045	25.182349
166.238899	5622.081441	25.187367
166.441260	5625.481816	25.192384
166.813079	5635.791844	25.197402
167.216768	5648.095901	25.202419
167.502352	5643.131779	25.207437
167.511489	5631.487484	25.212455
167.756471	5632.856788	25.217472
167.805701	5636.498720	25.222490
168.010902	5653.996220	25.227507
168.362631	5660.414322	25.232525
168.300587	5672.000408	25.237543
168.538074	5673.691114	25.242560
168.486793	5673.876409	25.247578
168.496819	5663.336530	25.252595
169.117482	5676.790062	25.257613
169.045870	5686.930869	25.262631
169.183864	5688.528083	25.267648
169.397147	5690.104639	25.272666
169.486242	5687.304686	25.277683
169.559791	5692.117359	25.282701
169.564835	5716.105992	25.287719
169.707749	5722.514144	25.292736
169.835080	5734.137745	25.297754
170.158338	5745.684486	25.302771
170.614351	5748.628261	25.307789
170.519623	5750.868379	25.312807
171.002375	5766.034695	25.317824
171.232005	5771.054598	25.322842
171.046941	5778.943796	25.327859
171.282321	5771.571540	25.332877
171.462907	5771.184881	25.337895
171.726961	5785.368037	25.342912
171.971096	5797.843993	25.347930
171.984035	5787.796851	25.352947
172.139911	5795.418492	25.357965
171.996817	5804.713222	25.362983
172.356054	5791.188516	25.368000
172.490164	5806.034393	25.373018
172.464398	5826.424028	25.378035
172.700120	5827.122945	25.383053
172.570241	5838.469790	25.388071
172.742167	5852.433247	25.393088
173.363007	5849.707408	25.398106
173.648081	5878.649880	25.403123
173.889234	5885.840207	25.408141
174.161836	5898.115022	25.413159
174.398672	5886.093559	25.418176
174.309183	5891.428731	25.423194
174.344785	5908.364295	25.428211
174.878239	5901.920812	25.433229
174.802495	5906.052427	25.438247
175.170414	5906.365218	25.443264
175.249691	5920.899745	25.448282
175.566072	5935.527873	25.453299
175.642897	5926.796918	25.458317
175.573137	5946.391244	25.463335
176.049837	5935.189849	25.468352
176.169485	5946.200387	25.473370
176.293487	5973.915426	25.478387
176.330102	5961.109171	25.483405
176.395035	5967.944483	25.488423
176.556366	5989.385516	25.493440
177.062520	5996.111158	25.498458
177.166480	5999.004902	25.503475
177.387385	5989.051135	25.508493
177.306493	6014.472476	25.513511
177.201914	6014.461715	25.518528
177.774238	6010.462742	25.523546
177.780477	6040.002290	25.528563
178.029399	6048.923116	25.533581
177.844008	6046.255762	25.538599
178.416537	6065.254544	25.543616
178.914389	6083.343172	25.548634
178.773506	6086.824343	25.553651
179.335455	6071.575524	25.558669
178.980710	6086.343845	25.563687
179.086169	6105.366005	25.568704
179.347709	6109.889998	25.573722
179.584309	6119.088198	25.578739
180.145333	6127.321247	25.583757
180.404565	6147.610814	25.588775
180.640729	6136.623853	25.593792
180.358754	6136.792433	25.598810
180.612698	6136.886585	25.603827
180.710332	6154.275159	25.608845
180.867464	6164.916398	25.613863
180.794894	6161.781792	25.618880
181.481378	6168.809993	25.623898
181.371510	6193.976628	25.628915
181.512193	6189.068473	25.633933
181.628546	6195.267065	25.638951
181.551279	6200.474516	25.643968
182.333019	6211.585828	25.648986
182.560079	6215.624407	25.654003
182.787946	6207.401063	25.659021
182.582609	6215.321260	25.664039
182.930442	6230.156307	25.669056
183.469751	6229.611741	25.674074
183.368673	6239.006258	25.679092
183.963333	6230.642599	25.684109
183.914766	6232.838452	25.689127
183.932612	6234.980444	25.694144
184.081689	6245.566378	25.699162
184.123763	6261.287328	25.704180
184.633860	6255.951260	25.709197
184.350252	6272.073470	25.714215
184.639401	6271.577440	25.719232
185.003253	6284.225909	25.724250
185.006333	6298.930311	25.729268
185.104800	6289.305852	25.734285
185.489696	6304.414369	25.739303
185.815253	6316.216895	25.744320
186.099799	6315.340798	25.749338
185.918976	6319.226498	25.754356
186.288820	6328.936233	25.759373
186.474096	6346.005005	25.764391
186.541094	6338.681344	25.769408
186.741939	6332.163249	25.774426
186.980283	6355.911950	25.779444
187.238958	6364.800729	25.784461
187.377789	6372.519799	25.789479
187.458198	6379.219869	25.794496
188.098267	6394.073793	25.799514
187.927777	6406.830373	25.804532
188.316736	6409.663026	25.809549
188.105144	6419.688177	25.814567
188.204717	6419.430076	25.819584
188.690543	6420.229197	25.824602
188.605695	6445.503207	25.829620
188.869042	6447.318129	25.834637
189.119943	6454.500886	25.839655
189.156066	6465.749360	25.844672
189.423212	6463.036533	25.849690
189.413370	6472.788013	25.854708
189.651589	6478.335509	25.859725
190.143333	6483.668709	25.864743
190.345886	6508.913530	25.869760
190.451398	6519.285519	25.874778
190.585428	6515.885798	25.879796
190.766087	6524.015275	25.884813
190.773927	6543.772685	25.889831
190.945741	6549.359906	25.894848
191.376301	6552.956218	25.899866
191.199051	6560.003508	25.904884
191.683316	6566.863512	25.909901
191.909775	6577.970790	25.914919
191.525455	6589.662473	25.919936
192.491129	6603.065789	25.924954
192.518331	6615.565221	25.929972
192.467892	6608.327028	25.934989
192.835781	6625.931924	25.940007
192.949198	6631.688991	25.945024
193.352366	6635.096141	25.950042
193.281901	6636.119291	25.955060
193.415223	6655.874942	25.960077
193.855816	6654.096676	25.965095
193.381450	6675.873728	25.970112
194.146072	6679.913282	25.975130
194.388045	6698.184296	25.980148
194.500511	6699.251459	25.985165
194.942381	6704.129269	25.990183
194.795182	6723.287707	25.995200
195.510219	6716.605642	26.000218
195.461065	6724.590905	26.005236
195.545400	6736.389737	26.010253
196.053172	6738.324661	26.015271
195.964034	6743.105390	26.020288
196.241616	6740.549783	26.025306
196.567393	6756.967192	26.030324
196.585058	6769.199190	26.035341
196.876155	6770.700517	26.040359
196.838357	6771.290450	26.045376
197.434201	6774.719632	26.050394
197.083102	6807.195788	26.055412
197.370018	6801.541049	26.060429
197.964413	6813.301114	26.065447
197.926332	6830.266789	26.070464
198.065276	6820.659925	26.075482
198.271275	6832.117635	26.080500
198.740920	6847.676626	26.085517
199.249724	6843.160407	26.090535
198.786185	6855.864166	26.095552
199.021956	6854.106730	26.100570
199.116596	6872.377057	26.105588
199.422099	6888.857642	26.110605
199.702159	6889.917771	26.115623
199.578260	6895.844958	26.120640
199.616289	6904.210607	26.125658
200.235387	6907.997258	26.130676
200.389825	6930.118193	26.135693
200.725129	6938.250783	26.140711
200.733488	6936.371443	26.145728
201.352884	6939.716656	26.150746
201.531625	6965.495573	26.155764
201.397370	6974.843914	26.160781
201.974256	6957.963119	26.165799
201.855716	6963.127847	26.170816
202.005692	6971.157817	26.175834
202.133539	6989.410406	26.180852
202.358347	6989.553275	26.185869
202.708192	7000.195866	26.190887
203.031035	7000.231049	26.195904
203.348445	7017.085975	26.200922
203.344369	7021.781633	26.205940
203.493444	7018.912858	26.210957
203.691799	7012.525474	26.215975
203.566354	7033.056976	26.220992
204.106162	7033.112647	26.226010
204.265816	7046.110623	26.231028
204.002326	7047.635088	26.236045
204.418549	7065.660830	26.241063
204.585082	7065.783878	26.246080
204.720751	7083.228851	26.251098
205.056112	7102.333664	26.256116
205.150212	7106.708413	26.261133
205.850134	7113.199898	26.266151
205.960986	7126.541695	26.271168
206.002218	7134.962828	26.276186
206.304916	7136.093328	26.281204
206.502409	7159.232965	26.286221
206.733686	7160.626635	26.291239
206.650535	7158.779952	26.296256
207.246086	7171.308843	26.301274
207.293014	7182.140698	26.306292
207.321040	7189.718136	26.311309
207.608207	7183.717012	26.316327
207.801830	7211.496443	26.321344
208.202307	7222.731468	26.326362
208.190788	7217.848027	26.331380
208.282216	7229.954556	26.336397
209.034269	7235.997164	26.341415
208.656083	7243.226305	26.346432
209.189747	7248.944943	26.351450
209.592367	7261.845363	26.356468
209.812440	7263.048844	26.361485
210.158097	7264.119788	26.366503
210.237436	7279.824861	26.371520
210.561940	7278.598501	26.376538
210.472051	7283.276448	26.381556
211.065054	7281.291273	26.386573
211.415038	7277.038654	26.391591
211.259400	7285.647835	26.396608
211.508048	7299.991482	26.401626
211.496158	7318.978832	26.406644
211.566582	7313.842313	26.411661
212.340046	7312.008549	26.416679
212.120411	7330.481399	26.421696
212.365442	7334.360845	26.426714
212.572139	7331.301854	26.431732
212.384735	7341.422908	26.436749
212.831503	7354.919870	26.441767
212.666432	7361.872749	26.446784
213.027728	7357.661580	26.451802
213.508430	7388.446902	26.456820
213.560484	7384.155984	26.461837
213.890939	7377.606543	26.466855
214.161429	7412.841909	26.471872
214.002957	7406.112319	26.476890
214.511249	7414.729823	26.481908
214.704230	7433.686233	26.486925
215.002895	7445.862976	26.491943
215.236328	7444.013786	26.496960
215.296195	7442.608501	26.501978
215.445736	7468.496809	26.506996
215.432574	7467.328985	26.512013
215.807247	7482.119312	26.517031
216.186174	7494.146391	26.522048
216.384898	7506.858429	26.527066
216.531422	7502.969440	26.532084
216.824981	7527.797842	26.537101
216.834180	7530.780170	26.542119
217.215542	7542.803753	26.547136
217.560329	7557.490335	26.552154
218.068635	7548.932778	26.557172
217.994109	7568.358472	26.562189
218.293620	7576.812645	26.567207
218.510211	7585.767883	26.572224
219.000552	7583.578721	26.577242
218.674352	7585.607371	26.582260
219.036229	7605.077242	26.587277
219.266624	7601.706763	26.592295
219.382641	7613.375348	26.597312
219.792728	7634.640624	26.602330
220.164612	7638.953937	26.607348
219.972784	7649.627483	26.612365
220.479403	7647.320838	26.617383
220.527909	7665.585333	26.622400
220.706340	7658.754709	26.627418
221.119929	7684.534419	26.632436
221.085044	7690.516187	26.637453
221.734594	7685.127489	26.642471
221.647119	7708.218989	26.647488
222.019785	7711.355861	26.652506
222.241627	7711.138050	26.657524
222.048326	7732.627124	26.662541
222.595263	7739.175541	26.667559
222.835966	7752.095120	26.672576
222.903089	7760.558118	26.677594
223.310653	7759.899964	26.682612
223.323730	7776.638244	26.687629
223.653035	7785.363186	26.692647
223.926949	7797.041365	26.697664
223.949506	7810.458441	26.702682
224.084750	7813.858223	26.707700
224.302034	7835.274124	26.712717
224.821936	7832.497156	26.717735
224.656922	7845.474412	26.722752
224.894460	7858.287577	26.727770
224.920352	7862.971641	26.732788
225.019431	7886.815027	26.737805
225.489549	7890.766538	26.742823
225.568570	7914.329896	26.747840
226.223621	7926.406159	26.752858
226.537818	7927.360207	26.757876
226.491773	7950.248762	26.762893
226.765968	7959.056556	26.767911
227.007265	7963.728346	26.772928
227.542061	7972.753483	26.777946
227.580221	7979.707300	26.782964
227.683545	7989.762775	26.787981
227.847224	8005.296223	26.792999
228.089867	7998.116071	26.798016
228.146903	8025.546610	26.803034
228.513449	8029.395852	26.808052
228.541306	8045.825989	26.813069
228.970338	8062.971976	26.818087
229.570273	8066.562127	26.823104
229.476225	8081.204302	26.828122
230.112997	8094.012256	26.833140
230.055161	8100.409378	26.838157
230.823714	8102.504362	26.843175
230.702028	8123.437281	26.848192
230.931730	8129.738220	26.853210
231.154350	8121.001623	26.858228
231.254200	8141.232774	26.863245
231.507629	8156.981053	26.868263
231.818815	8157.609833	26.873280
231.864985	8173.288088	26.878298
232.138207	8177.453619	26.883316
232.089228	8201.103932	26.888333
232.379023	8212.061492	26.893351
232.645469	8224.040211	26.898368
232.770138	8239.797300	26.903386
233.252340	8242.659517	26.908404
233.188421	8263.179756	26.913421
233.447493	8265.477160	26.918439
234.142427	8274.852296	26.923456
234.325559	8300.188242	26.928474
234.575915	8299.744766	26.933492
235.186753	8306.486266	26.938509
235.668702	8308.519953	26.943527
235.987945	8331.311519	26.948544
235.986430	8335.807315	26.953562
236.438884	8326.091278	26.958580
236.547514	8323.210605	26.963597
236.474960	8334.725685	26.968615
236.349613	8319.481854	26.973632
236.697510	8329.536342	26.978650
236.798015	8340.193681	26.983668
237.059490	8347.449643	26.988685
237.244252	8350.690575	26.993703
237.334614	8375.488259	26.998720
237.576552	8384.126761	27.003738
238.326057	8377.111138	27.008756
237.917392	8404.624480	27.013773
238.080592	8406.180205	27.018791
238.303689	8420.053730	27.023808
238.481381	8436.465133	27.028826
238.922120	8429.789067	27.033844
239.145555	8465.238230	27.038861
239.594046	8472.587590	27.043879
239.683604	8478.974362	27.048896
239.819763	8487.148996	27.053914
240.628747	8484.515866	27.058932
240.451194	8499.284287	27.063949
240.702896	8520.131093	27.068967
241.073048	8522.253453	27.073984
241.310123	8535.814823	27.079002
241.840400	8549.325532	27.084020
241.663433	8568.110227	27.089037
242.029043	8559.939572	27.094055
242.436705	8580.084480	27.099072
242.260194	8594.496758	27.104090
242.965897	8591.309183	27.109108
242.940297	8611.436639	27.114125
243.284416	8612.518164	27.119143
243.143213	8620.060748	27.124160
243.550411	8639.685672	27.129178
243.835191	8643.556767	27.134196
243.710598	8663.970374	27.139213
244.089691	8669.737425	27.144231
244.388448	8684.336067	27.149248
244.728299	8696.798820	27.154266
245.186753	8711.169798	27.159284
245.496500	8725.071894	27.164301
245.783935	8732.288890	27.169319
246.093932	8743.360083	27.174336
246.448440	8764.301011	27.179354
246.359305	8760.436279	27.184372
246.512875	8770.465386	27.189389
246.744056	8774.567361	27.194407
246.892789	8791.925302	27.199424
247.152634	8805.363678	27.204442
247.562630	8810.952347	27.209460
247.868381	8834.600233	27.214477
248.037828	8831.618881	27.219495
248.481134	8849.326142	27.224512
248.556109	8852.049193	27.229530
249.202842	8869.542275	27.234548
249.517900	8872.960066	27.239565
249.351920	8873.857342	27.244583
249.907068	8881.638837	27.249600
250.078627	8890.187340	27.254618
250.263307	8905.853336	27.259636
250.394736	8910.167976	27.264653
250.521864	8917.316973	27.269671
250.596681	8932.553150	27.274688
250.698275	8941.577507	27.279706
250.957619	8953.332103	27.284724
250.921717	8969.432291	27.289741
251.239909	8992.650757	27.294759
251.826115	8996.337368	27.299776
251.855865	9019.727367	27.304794
252.142985	9022.533884	27.309812
252.385278	9041.722130	27.314829
252.837459	9054.594968	27.319847
253.004437	9065.182423	27.324864
253.134709	9077.389316	27.329882
253.926102	9078.219771	27.334900
254.264032	9102.222575	27.339917
254.263071	9120.602970	27.344935
254.662576	9105.307725	27.349952
254.668125	9134.687484	27.354970
255.093388	9140.498117	27.359988
255.445686	9139.054324	27.365005
255.376185	9160.655161	27.370023
255.536602	9168.916406	27.375040
255.526609	9171.531086	27.380058
256.098153	9188.874030	27.385076
256.255855	9208.612658	27.390093
256.465934	9222.625144	27.395111
256.952112	9230.643273	27.400128
257.091020	9253.089236	27.405146
257.305295	9268.108365	27.410164
257.652949	9274.937120	27.415181
257.629013	9279.041734	27.420199
258.417080	9311.952402	27.425216
258.359006	9326.054944	27.430234
258.958395	9336.816828	27.435252
259.309632	9348.042433	27.440269
258.668624	9353.192503	27.445287
259.555193	9369.407736	27.450304
259.553845	9382.239831	27.455322
259.709569	9401.301870	27.460340
260.338176	9413.210442	27.465357
260.974246	9432.225858	27.470375
261.022329	9441.341281	27.475392
260.897742	9443.315213	27.480410
261.591754	9470.267959	27.485428
262.014467	9462.795570	27.490445
261.717579	9484.063649	27.495463
262.154188	9494.809493	27.500480
262.460786	9506.183195	27.505498
262.886351	9507.894742	27.510516
263.232351	9527.070229	27.515533
263.239660	9530.467584	27.520551
263.672136	9560.982970	27.525568
263.534791	9563.874169	27.530586
263.710331	9576.238332	27.535604
264.324304	9585.803881	27.540621
264.231947	9601.529716	27.545639
264.926351	9609.508172	27.550656
264.771631	9631.358961	27.555674
265.065070	9639.362391	27.560692
265.448850	9645.487534	27.565709
266.146083	9646.734383	27.570727
265.816144	9665.293401	27.575744
265.906366	9684.202162	27.580762
266.104244	9688.498961	27.585780
266.533133	9703.599608	27.590797
266.489951	9720.907768	27.595815
267.194866	9741.206358	27.600832
267.433230	9747.981925	27.605850
267.595811	9768.943050	27.610868
268.264482	9774.208729	27.615885
268.235120	9806.169503	27.620903
268.938397	9798.281571	27.625920
268.660033	9828.278880	27.630938
269.211463	9827.093672	27.635956
269.324955	9850.025018	27.640973
269.601222	9868.106771	27.645991
270.151033	9869.382648	27.651008
270.009819	9886.716462	27.656026
270.355259	9894.497293	27.661044
270.745606	9914.016013	27.666061
271.113434	9921.016556	27.671079
271.530000	9935.178586	27.676096
271.549411	9961.970999	27.681114
271.772220	9960.416742	27.686132
272.363523	9981.070589	27.691149
272.229670	9994.612531	27.696167
272.827349	10004.382020	27.701184
272.719872	10012.324819	27.706202
273.167783	10030.550969	27.711220
273.465773	10037.825153	27.716237
273.727814	10067.656924	27.721255
274.125665	10068.458494	27.726272
273.830371	10097.088523	27.731290
274.276056	10112.556785	27.736308
274.840937	10121.713410	27.741325
274.981109	10144.730669	27.746343
275.340601	10149.651883	27.751360
275.529609	10167.409112	27.756378
276.030753	10181.091217	27.761396
276.415535	10198.021643	27.766413
276.609418	10198.576354	27.771431
277.031000	10227.258420	27.776448
277.073634	10228.686392	27.781466
277.217451	10248.638727	27.786484
277.551500	10254.070848	27.791501
277.582067	10284.829234	27.796519
278.018025	10290.505617	27.801536
278.365500	10317.330186	27.806554
278.786133	10322.911044	27.811572
279.025755	10336.406749	27.816589
279.228809	10354.984362	27.821607
279.981062	10350.307908	27.826624
279.998136	10364.687876	27.831642
279.962312	10386.799010	27.836660
280.445401	10387.359180	27.841677
280.550979	10394.065702	27.846695
280.980447	10404.681915	27.851712
280.848217	10423.117880	27.856730
281.454213	10431.393010	27.861748
281.737750	10439.729772	27.866765
281.988954	10460.232298	27.871783
282.384155	10462.632697	27.876800
282.731852	10476.864062	27.881818
282.953404	10498.109567	27.886836
283.519305	10508.234273	27.891853
283.377822	10509.997759	27.896871
283.767423	10517.206422	27.901888
283.941591	10529.237904	27.906906
284.160123	10542.788311	27.911924
284.317803	10558.934899	27.916941
284.695510	10578.030340	27.921959
285.192408	10588.382129	27.926976
285.216049	10600.178738	27.931994
285.555414	10611.088844	27.937012
286.145707	10638.281377	27.942029
286.324995	10653.607321	27.947047
286.369860	10660.250841	27.952064
286.956773	10676.612462	27.957082
287.088012	10683.727807	27.962100
287.291788	10713.506399	27.967117
287.672624	10721.738879	27.972135
288.220680	10738.064262	27.977152
288.470784	10743.070005	27.982170
288.358018	10762.690483	27.987188
289.123378	10767.695565	27.992205
289.047080	10787.298457	27.997223
289.275136	10797.479175	28.002240
289.740155	10815.651218	28.007258
289.951017	10832.245302	28.012276
290.180281	10838.143329	28.017293
290.289664	10873.468407	28.022311
290.727000	10870.986606	28.027328
291.091257	10898.216621	28.032346
291.142639	10912.173738	28.037364
291.738478	10937.140640	28.042381
291.615563	10938.990937	28.047399
291.985006	10964.505137	28.052416
292.502182	10971.180156	28.057434
292.791216	10990.865567	28.062452
293.319711	11012.313148	28.067469
293.372869	11021.125324	28.072487
293.746561	11041.437550	28.077504
294.019537	11055.996184	28.082522
294.185586	11066.847674	28.087540
294.463253	11084.120034	28.092557
294.872687	11110.432841	28.097575
295.237464	11111.114609	28.102592
295.362031	11123.440950	28.107610
295.759023	11142.830352	28.112628
295.992080	11155.273222	28.117645
296.064892	11158.861197	28.122663
296.666290	11182.806058	28.127680
296.811242	11182.662642	28.132698
296.787960	11206.635485	28.137716
297.331117	11205.892239	28.142733
297.573701	11239.504039	28.147751
297.771205	11245.668584	28.152768
298.197132	11266.650425	28.157786
298.425494	11281.303748	28.162804
298.985724	11298.896110	28.167821
299.041710	11313.248744	28.172839
299.190153	11340.964339	28.177856
299.765873	11348.597074	28.182874
299.783064	11362.806401	28.187892
300.483478	11382.838773	28.192909
300.568844	11398.100166	28.197927
300.982473	11421.768782	28.202944
301.214688	11437.958738	28.207962
301.706761	11455.717982	28.212980
302.245155	11457.311828	28.217997
302.166291	11479.565219	28.223015
302.636311	11492.687206	28.228032
303.225900	11503.882346	28.233050
303.444698	11519.535794	28.238068
303.559620	11528.075548	28.243085
304.134558	11546.742540	28.248103
304.079133	11554.350832	28.253120
304.534099	11570.649853	28.258138
304.427172	11585.087345	28.263156
305.100707	11590.642148	28.268173
305.342537	11613.144490	28.273191
305.797678	11626.730572	28.278208
306.107701	11629.393844	28.283226
306.011504	11653.353043	28.288244
306.402502	11668.370414	28.293261
306.983481	11676.676987	28.298279
307.295281	11693.839929	28.303296
307.462417	11706.753009	28.308314
307.633760	11718.205437	28.313332
307.986401	11738.555803	28.318349
308.184885	11764.132252	28.323367
308.270949	11780.799019	28.328384
308.832340	11791.787150	28.333402
308.831274	11814.018400	28.338420
309.376386	11828.805552	28.343437
309.609898	11854.102082	28.348455
309.807392	11886.093281	28.353472
310.354759	11895.014130	28.358490
310.471233	11908.577114	28.363508
311.197115	11929.400112	28.368525
311.589592	11947.112254	28.373543
311.807261	11964.500260	28.378560
312.061633	11970.475603	28.383578
312.201941	11989.671671	28.388596
312.595041	11995.394499	28.393613
313.064203	12004.965406	28.398631
313.220450	12019.657111	28.403648
313.739110	12030.353336	28.408666
314.091066	12049.313076	28.413684
314.648090	12036.265210	28.418701
314.622768	12073.147782	28.423719
314.567715	12086.324260	28.428736
315.286301	12082.631981	28.433754
315.567363	12100.972243	28.438772
315.878606	12104.277662	28.443789
316.014886	12124.674050	28.448807
316.279391	12142.318468	28.453824
316.743761	12155.486800	28.458842
316.557003	12175.455605	28.463860
316.976936	12188.427193	28.468877
317.517193	12210.623716	28.473895
317.668497	12225.446080	28.478912
318.102552	12235.443034	28.483930
318.273685	12265.651373	28.488948
318.677024	12289.039837	28.493965
319.147199	12308.157762	28.498983
319.214718	12327.152361	28.504000
319.433373	12356.572514	28.509018
319.708399	12381.616556	28.514036
320.255540	12383.578655	28.519053
320.379320	12394.680655	28.524071
320.818720	12438.338157	28.529088
321.234146	12450.791994	28.534106
321.547891	12478.567743	28.539124
321.851332	12497.400593	28.544141
322.276286	12524.892075	28.549159
322.454137	12538.791772	28.554176
323.033988	12547.690321	28.559194
323.332127	12572.106429	28.564212
323.736171	12584.629488	28.569229
324.318919	12605.108853	28.574247
324.304147	12616.185477	28.579264
325.168525	12622.512906	28.584282
325.375769	12652.048992	28.589300
325.320410	12659.543697	28.594317
325.792011	12675.313113	28.599335
325.867600	12684.541031	28.604352
326.325810	12712.007087	28.609370
326.808227	12724.900308	28.614388
327.135328	12731.233715	28.619405
327.568470	12746.345013	28.624423
327.798409	12766.058293	28.629440
328.189484	12772.468105	28.634458
328.536191	12785.936739	28.639476
328.507297	12809.814228	28.644493
328.989390	12815.842954	28.649511
329.055450	12826.006192	28.654528
329.452020	12842.512675	28.659546
329.518794	12862.646036	28.664564
329.960548	12886.824093	28.669581
330.208961	12890.831972	28.674599
330.207916	12916.718247	28.679616
330.467011	12926.644760	28.684634
330.932184	12959.548375	28.689652
331.377389	12985.872524	28.694669
331.610969	13006.220548	28.699687
332.003760	13032.149335	28.704704
332.227267	13053.026008	28.709722
332.195616	13079.851759	28.714740
332.747953	13108.402758	28.719757
333.602338	13126.275266	28.724775
333.498474	13154.457076	28.729792
333.902655	13169.277451	28.734810
334.393441	13186.724678	28.739828
334.554810	13208.433038	28.744845
334.977285	13248.342113	28.749863
335.303288	13282.157284	28.754880
335.920430	13284.988963	28.759898
336.310896	13312.006820	28.764916
336.713818	13328.747978	28.769933
337.202062	13342.695568	28.774951
337.447815	13380.226759	28.779968
338.054234	13380.902408	28.784986
338.344718	13394.869459	28.790004
338.263556	13407.069278	28.795021
338.698383	13424.598507	28.800039
339.056189	13447.082335	28.805056
339.580853	13458.665835	28.810074
339.954596	13493.845868	28.815092
339.885027	13501.986943	28.820109
340.489441	13516.768959	28.825127
340.340591	13540.653033	28.830144
341.144025	13562.121135	28.835162
341.478215	13579.873505	28.840180
341.605394	13604.278374	28.845197
342.178388	13629.839019	28.850215
342.480766	13647.903825	28.855232
342.758152	13654.715378	28.860250
343.191898	13677.590372	28.865268
343.427163	13701.559107	28.870285
343.959556	13717.423730	28.875303
344.196610	13728.858842	28.880320
344.562546	13757.470188	28.885338
344.978929	13759.996680	28.890356
345.160598	13791.493680	28.895373
345.514823	13809.607879	28.900391
345.760275	13830.428889	28.905408
346.243902	13845.285381	28.910426
346.390922	13867.882139	28.915444
346.591144	13887.236263	28.920461
347.573473	13912.796996	28.925479
347.665923	13927.201981	28.930496
348.127685	13929.759621	28.935514
348.361948	13956.488843	28.940532
348.731190	13959.231458	28.945549
349.126142	13978.285354	28.950567
349.558289	13992.563355	28.955584
349.963199	14001.445286	28.960602
350.100056	14012.428898	28.965620
350.480233	14029.313589	28.970637
351.217020	14031.506348	28.975655
351.443003	14048.685045	28.980672
351.457273	14073.475483	28.985690
351.740242	14086.594804	28.990708
351.954295	14107.112819	28.995725
352.425658	14118.480284	29.000743
352.573919	14142.892298	29.005760
352.692847	14160.167980	29.010778
352.747204	14180.714790	29.015796
353.044410	14214.022883	29.020813
353.720752	14226.765353	29.025831
354.183400	14259.945142	29.030848
354.250908	14285.129496	29.035866
354.572473	14301.185765	29.040884
355.403528	14336.206800	29.045901
355.738003	14356.041075	29.050919
355.545647	14390.553453	29.055936
356.450771	14416.523693	29.060954
356.838853	14437.425336	29.065972
357.094314	14467.678824	29.070989
357.711422	14489.144773	29.076007
358.282521	14506.635037	29.081024
358.289894	14528.368144	29.086042
358.792489	14541.576646	29.091060
359.050473	14570.471025	29.096077
359.233329	14594.061791	29.101095
359.424257	14618.934874	29.106112
359.955011	14642.297310	29.111130
360.550446	14664.688192	29.116148
360.708221	14688.211685	29.121165
361.220868	14714.453687	29.126183
361.985243	14728.981334	29.131200
362.198257	14746.188565	29.136218
362.382900	14756.026391	29.141236
362.699191	14788.702726	29.146253
363.502258	14793.747461	29.151271
363.678947	14831.606441	29.156288
364.001090	14830.856157	29.161306
364.404452	14845.838696	29.166324
364.201853	14873.744002	29.171341
364.847187	14889.342107	29.176359
365.423423	14918.749883	29.181376
365.416817	14938.329594	29.186394
366.374665	14955.759630	29.191412
366.524050	14996.919581	29.196429
366.925538	14990.187987	29.201447
367.154200	15019.318150	29.206464
367.352722	15019.192740	29.211482
367.564768	15046.478863	29.216500
367.695082	15063.720983	29.221517
368.463104	15080.151714	29.226535
368.811206	15110.098860	29.231552
369.080718	15115.417566	29.236570
369.524760	15141.255477	29.241588
369.747884	15165.273514	29.246605
370.465299	15174.875464	29.251623
370.796199	15202.645969	29.256640
371.039098	15210.216909	29.261658
371.534651	15225.574420	29.266676
371.517374	15256.407956	29.271693
372.060775	15266.828576	29.276711
372.545848	15280.875088	29.281728
372.969443	15319.287343	29.286746
373.648184	15319.957970	29.291764
373.530822	15343.983506	29.296781
374.084240	15360.120358	29.301799
374.217302	15392.863491	29.306816
374.591136	15409.643951	29.311834
375.422748	15437.880658	29.316852
375.352420	15474.168396	29.321869
375.831671	15482.315176	29.326887
376.302642	15504.238143	29.331904
376.366530	15530.016247	29.336922
376.849776	15560.368151	29.341940
376.859503	15592.049967	29.346957
377.575141	15599.493908	29.351975
377.831339	15636.067041	29.356992
378.358561	15666.128241	29.362010
378.860281	15685.697576	29.367028
378.929106	15708.911276	29.372045
379.476521	15726.809106	29.377063
380.217893	15757.929971	29.382080
380.683810	15776.481090	29.387098
380.905556	15794.019153	29.392116
381.067173	15815.447956	29.397133
381.619990	15839.916003	29.402151
381.788560	15863.095049	29.407168
382.065969	15892.112327	29.412186
382.458515	15918.656985	29.417204
382.627480	15949.838747	29.422221
383.374553	15968.664833	29.427239
383.989038	16001.670292	29.432256
384.018646	16019.201734	29.437274
384.457891	16046.247950	29.442292
384.802626	16069.082354	29.447309
385.586104	16089.276596	29.452327
386.024061	16118.282693	29.457344
386.066165	16140.221864	29.462362
387.104226	16157.969882	29.467380
387.137695	16181.937753	29.472397
387.789894	16188.539462	29.477415
387.848860	16207.044646	29.482432
388.157974	16210.158625	29.487450
389.008559	16228.211362	29.492468
389.252904	16249.613614	29.497485
389.217695	16264.622356	29.502503
389.705136	16271.494612	29.507520
389.838808	16295.972015	29.512538
390.459598	16308.416174	29.517556
390.511906	16341.924290	29.522573
390.689448	16368.728167	29.527591
391.286166	16380.796152	29.532608
391.640034	16402.108143	29.537626
392.153373	16429.950407	29.542644
392.167595	16459.743277	29.547661
392.944311	16474.280569	29.552679
393.009247	16515.684882	29.557696
393.375917	16528.663746	29.562714
394.137392	16560.162716	29.567732
394.290702	16595.433028	29.572749
394.596316	16608.787000	29.577767
395.204614	16648.794219	29.582784
395.254226	16679.019815	29.587802
395.882048	16702.963664	29.592820
396.536220	16720.158024	29.597837
397.079630	16744.241555	29.602855
397.648428	16777.773425	29.607872
397.849394	16792.444686	29.612890
398.454866	16804.815320	29.617908
398.739237	16824.570431	29.622925
398.834949	16861.122051	29.627943
399.326557	16876.480275	29.632960
400.034346	16904.605967	29.637978
400.516776	16927.734439	29.642996
400.481969	16958.101775	29.648013
400.765052	16982.274203	29.653031
401.131687	16996.566930	29.658048
401.349196	17034.096705	29.663066
402.308420	17047.395728	29.668084
402.472731	17083.215155	29.673101
402.522777	17106.647023	29.678119
403.632188	17125.835663	29.683136
403.873199	17157.248721	29.688154
404.473613	17183.470338	29.693172
404.738261	17199.958072	29.698189
405.188855	17222.206695	29.703207
405.793998	17243.728809	29.708224
405.773791	17277.774484	29.713242
406.449170	17283.801959	29.718260
406.545943	17313.841766	29.723277
407.136895	17331.075033	29.728295
407.605892	17364.768364	29.733312
407.809345	17383.068088	29.738330
408.285495	17399.783736	29.743348
408.548876	17437.863051	29.748365
408.684382	17457.136424	29.753383
409.316330	17471.244611	29.758400
409.400970	17509.842317	29.763418
410.197748	17523.631195	29.768436
410.302085	17564.332471	29.773453
410.863879	17583.995535	29.778471
411.503091	17606.772897	29.783488
411.458764	17625.760190	29.788506
411.979127	17650.457638	29.793524
412.295332	17685.920220	29.798541
412.817907	17708.499398	29.803559
413.499995	17726.534888	29.808576
413.511996	17757.243167	29.813594
414.425843	17774.312692	29.818612
414.527244	17803.494282	29.823629
414.931362	17827.406630	29.828647
415.355038	17856.092498	29.833664
415.811510	17885.464902	29.838682
416.199436	17906.885550	29.843700
416.329611	17930.563368	29.848717
416.535392	17960.102231	29.853735
417.307210	17995.804336	29.858752
417.649795	18028.179329	29.863770
418.172921	18064.703482	29.868788
418.506133	18090.395605	29.873805
418.787226	18121.332588	29.878823
419.478299	18146.690625	29.883840
419.752973	18197.186726	29.888858
420.552353	18216.963134	29.893876
420.741078	18239.177782	29.898893
421.304523	18269.928344	29.903911
421.976963	18281.761357	29.908928
421.947081	18318.179338	29.913946
422.423275	18332.453092	29.918964
423.332033	18364.703933	29.923981
423.452988	18394.991389	29.928999
424.257823	18415.138048	29.934016
424.791377	18429.761808	29.939034
425.200089	18455.365341	29.944052
425.237914	18467.839769	29.949069
425.970467	18494.302796	29.954087
426.772579	18514.912620	29.959104
426.965246	18532.399865	29.964122
427.247327	18555.725691	29.969140
427.558064	18576.185145	29.974157
427.981402	18601.761786	29.979175
428.557319	18619.806577	29.984192
428.807076	18652.790979	29.989210
429.191700	18682.963363	29.994228
429.539847	18705.732816	29.999245
429.672822	18728.878718	30.004263
430.275800	18747.715032	30.009280
430.376334	18790.522533	30.014298
431.212526	18816.066820	30.019316
431.531422	18838.926170	30.024333
432.343658	18867.598460	30.029351
432.985348	18889.245397	30.034368
433.075961	18904.077585	30.039386
433.751279	18910.415571	30.044404
433.988150	18943.277441	30.049421
434.195356	18947.354512	30.054439
434.894290	18964.618270	30.059456
435.183161	18988.743693	30.064474
435.372127	19004.484750	30.069492
435.942629	19038.159839	30.074509
436.263436	19051.997974	30.079527
436.793163	19068.808866	30.084544
437.473934	19100.095162	30.089562
437.973942	19106.639910	30.094580
438.257442	19131.540854	30.099597
437.849827	19155.311338	30.104615
438.818143	19182.287218	30.109632
439.376367	19213.698785	30.114650
439.702102	19248.347627	30.119668
440.322840	19269.844096	30.124685
440.723638	19296.456238	30.129703
441.178709	19320.719878	30.134720
441.680292	19355.624817	30.139738
442.297963	19369.492714	30.144756
442.404681	19398.031526	30.149773
442.419706	19424.169882	30.154791
443.123812	19445.954907	30.159808
443.568862	19476.812557	30.164826
443.780823	19515.494173	30.169844
444.289571	19545.704758	30.174861
444.598828	19575.845603	30.179879
445.235481	19599.072799	30.184896
445.579407	19647.971506	30.189914
446.241186	19671.236543	30.194932
446.946559	19696.049914	30.199949
447.334594	19743.261440	30.204967
447.783694	19759.402404	30.209984
448.253033	19791.584875	30.215002
448.623056	19821.848415	30.220020
449.273824	19836.011484	30.225037
449.948145	19861.195848	30.230055
450.291904	19885.786400	30.235072
450.662173	19916.916703	30.240090
450.992891	19933.001897	30.245108
451.481815	19968.712666	30.250125
451.442604	19998.368846	30.255143
452.206700	20031.348244	30.260160
452.985485	20055.599255	30.265178
452.926100	20091.240557	30.270196
453.064694	20116.974514	30.275213
453.967597	20162.119235	30.280231
454.530332	20173.278190	30.285248
454.829685	20223.381209	30.290266
455.395304	20243.696724	30.295284
455.551401	20276.099410	30.300301
455.996557	20297.032683	30.305319
456.528123	20309.955182	30.310336
456.938400	20355.469925	30.315354
457.275228	20379.530797	30.320372
457.894936	20402.718580	30.325389
458.580655	20432.827483	30.330407
459.017485	20447.954843	30.335424
459.358375	20487.993699	30.340442
459.880674	20495.312362	30.345460
460.542415	20524.893303	30.350477
460.916353	20560.344571	30.355495
461.202230	20570.662760	30.360512
461.772129	20604.203122	30.365530
461.655255	20631.071296	30.370548
462.598550	20660.587950	30.375565
462.497068	20697.321742	30.380583
463.494548	20723.417574	30.385600
463.930413	20753.554301	30.390618
464.397798	20788.789594	30.395636
465.227264	20822.409168	30.400653
465.039278	20843.933093	30.405671
465.793200	20876.474098	30.410688
466.346482	20904.493654	30.415706
466.789651	20932.183502	30.420724
467.355191	20957.616533	30.425741
467.908521	20978.198786	30.430759
468.409817	21012.474299	30.435776
468.645790	21043.115947	30.440794
469.196492	21065.230487	30.445812
469.780121	21090.314336	30.450829
469.764341	21121.341972	30.455847
470.490513	21148.032621	30.460864
471.467465	21177.053861	30.465882
472.007758	21202.665359	30.470900
472.537369	21219.878667	30.475917
472.621589	21251.819143	30.480935
473.166180	21279.531250	30.485952
473.465694	21295.043185	30.490970
473.639468	21338.808761	30.495988
474.545747	21365.542756	30.501005
474.811409	21405.307300	30.506023
475.093543	21431.179238	30.511040
475.584850	21460.965907	30.516058
475.934330	21500.353488	30.521076
476.464423	21535.302854	30.526093
477.316805	21576.116321	30.531111
477.382755	21593.948111	30.536128
477.830499	21639.352320	30.541146
478.080371	21674.779010	30.546164
478.863781	21705.786801	30.551181
479.152459	21743.884405	30.556199
479.972151	21775.250411	30.561216
480.587644	21801.306123	30.566234
480.811318	21848.159533	30.571252
481.504921	21877.578471	30.576269
481.510843	21918.751345	30.581287
482.269449	21949.265033	30.586304
482.684833	21973.652525	30.591322
482.990068	22007.577892	30.596340
483.739884	22026.836225	30.601357
484.007007	22063.189600	30.606375
484.612665	22093.112042	30.611392
485.328247	22121.224479	30.616410
485.499338	22146.955403	30.621428
486.157312	22181.221895	30.626445
486.282240	22212.968810	30.631463
487.045568	22237.600568	30.636480
487.087736	22273.034125	30.641498
487.608396	22323.576413	30.646516
488.222341	22344.658805	30.651533
488.722254	22389.763092	30.656551
489.363438	22431.052692	30.661568
489.997212	22458.985803	30.666586
490.291374	22497.423023	30.671604
490.877015	22520.838325	30.676621
491.069610	22564.406613	30.681639
491.745540	22596.099602	30.686656
492.469195	22632.943917	30.691674
492.718104	22661.269494	30.696692
493.741361	22692.932552	30.701709
494.178894	22730.539406	30.706727
494.429094	22760.603228	30.711744
495.322230	22795.181723	30.716762
495.709051	22814.965121	30.721780
495.943878	22846.195661	30.726797
496.648013	22878.225766	30.731815
497.188458	22912.378674	30.736832
497.718794	22932.344929	30.741850
497.930924	22967.232343	30.746868
498.712570	23001.102067	30.751885
499.489524	23042.087304	30.756903
500.003374	23067.374459	30.761920
500.142064	23099.194998	30.766938
500.396939	23125.884536	30.771956
501.246608	23150.155835	30.776973
501.786790	23193.343613	30.781991
502.293142	23209.103311	30.787008
503.056858	23249.277561	30.792026
503.150785	23282.532022	30.797044
503.595705	23304.079768	30.802061
504.015753	23351.019771	30.807079
504.294594	23374.606513	30.812096
505.062459	23407.284440	30.817114
505.742110	23437.143298	30.822132
506.467825	23474.677660	30.827149
506.531933	23503.932897	30.832167
506.775527	23534.209545	30.837184
507.367442	23572.826428	30.842202
507.514732	23619.913071	30.847220
508.245340	23646.360719	30.852237
509.013603	23693.226575	30.857255
509.480397	23721.012082	30.862272
509.973045	23752.663336	30.867290
510.460496	23789.732291	30.872308
510.872061	23815.133031	30.877325
511.045251	23853.724353	30.882343
511.644784	23889.439004	30.887360
512.460178	23919.029819	30.892378
512.806264	23957.576524	30.897396
512.936570	23978.761774	30.902413
513.321651	24024.627066	30.907431
514.000900	24067.459521	30.912448
514.523355	24104.392879	30.917466
514.923357	24137.496398	30.922484
515.947968	24190.744121	30.927501
516.349927	24225.808073	30.932519
517.040335	24261.595733	30.937536
517.575654	24293.813135	30.942554
517.835125	24333.268581	30.947572
518.478849	24362.331456	30.952589
518.761460	24406.080294	30.957607
519.328928	24453.543586	30.962624
520.154470	24486.282295	30.967642
520.557324	24520.010806	30.972660
521.267672	24540.378143	30.977677
521.815431	24583.288861	30.982695
522.230543	24623.047920	30.987712
522.999053	24653.684992	30.992730
523.425296	24695.030488	30.997748
523.946653	24723.849632	31.002765
524.338288	24764.758125	31.007783
524.737169	24799.607997	31.012800
525.356426	24836.282654	31.017818
525.645813	24883.316525	31.022836
526.534373	24907.949835	31.027853
527.050312	24958.525692	31.032871
527.720345	24990.841207	31.037888
528.340195	25018.031136	31.042906
528.760681	25064.438106	31.047924
529.254043	25090.205966	31.052941
529.850944	25111.594895	31.057959
530.175398	25154.706570	31.062976
530.921001	25197.989176	31.067994
531.619622	25230.064301	31.073012
532.171383	25260.833173	31.078029
532.318258	25299.990697	31.083047
532.829059	25335.021636	31.088064
533.738756	25371.979755	31.093082
533.965046	25406.421243	31.098100
534.610538	25441.540459	31.103117
535.084882	25480.170461	31.108135
535.512272	25521.072834	31.113152
536.174456	25543.211341	31.118170
536.659029	25593.409779	31.123188
537.113907	25625.878229	31.128205
537.708573	25655.629544	31.133223
538.026784	25697.164999	31.138240
538.817386	25721.533156	31.143258
539.287816	25759.968304	31.148276
539.819387	25785.711508	31.153293
540.067341	25825.473403	31.158311
540.497974	25863.949014	31.163328
540.953306	25896.981988	31.168346
541.371244	25947.316617	31.173364
542.200811	25979.096670	31.178381
542.633664	26015.449229	31.183399
542.772317	26059.706857	31.188416
543.643490	26098.567412	31.193434
544.141840	26142.695501	31.198452
544.616426	26179.784667	31.203469
545.405205	26222.969427	31.208487
545.789735	26272.287846	31.213504
546.424426	26306.646524	31.218522
546.754404	26352.527278	31.223540
547.552837	26383.565476	31.228557
548.155723	26432.917360	31.233575
548.743286	26482.120578	31.238592
549.551275	26512.227895	31.243610
550.063348	26555.281156	31.248628
550.672934	26587.119515	31.253645
551.437208	26628.130193	31.258663
551.847417	26669.321844	31.263680
552.386782	26703.017462	31.268698
552.914402	26740.982618	31.273716
553.574176	26780.442577	31.278733
554.240342	26808.994256	31.283751
554.362202	26857.807987	31.288768
555.065519	26890.348149	31.293786
555.576544	26928.873384	31.298804
556.152000	26968.182578	31.303821
556.608898	27007.541477	31.308839
556.670925	27053.531511	31.313856
557.661718	27087.197001	31.318874
558.323615	27137.009622	31.323892
559.013948	27185.565994	31.328909
559.589847	27231.610986	31.333927
559.575720	27281.049567	31.338944
560.591485	27310.126307	31.343962
561.049346	27360.352645	31.348980
561.683251	27399.710309	31.353997
562.316455	27435.215597	31.359015
562.828062	27481.514988	31.364032
563.502449	27517.366855	31.369050
563.720310	27564.666573	31.374068
564.358843	27599.493818	31.379085
565.130657	27652.581408	31.384103
565.181349	27702.222888	31.389120
565.933783	27730.554469	31.394138
566.781331	27768.550669	31.399156
567.275202	27823.299791	31.404173
567.899041	27852.124789	31.409191
568.326681	27898.976079	31.414208
568.887193	27927.804997	31.419226
569.337990	27971.558041	31.424244
570.054699	28001.159543	31.429261
570.755025	28032.214981	31.434279
571.352098	28080.706964	31.439296
572.096279	28104.376264	31.444314
572.649642	28144.062151	31.449332
573.053501	28177.760378	31.454349
574.104667	28211.185396	31.459367
574.640754	28258.606646	31.464384
574.953167	28267.248992	31.469402
575.102202	28320.444272	31.474420
575.803463	28358.737774	31.479437
576.506382	28384.683195	31.484455
576.665994	28436.619689	31.489472
577.693900	28464.732202	31.494490
578.038892	28505.221152	31.499508
578.585836	28549.753079	31.504525
579.140233	28585.456244	31.509543
579.614109	28629.977967	31.514560
580.774669	28666.286008	31.519578
581.132747	28707.876455	31.524596
581.679437	28739.280767	31.529613
582.663948	28779.071312	31.534631
582.713127	28824.869871	31.539648
583.467696	28863.660347	31.544666
584.152885	28910.382149	31.549684
584.355709	28962.070763	31.554701
585.175501	29000.479279	31.559719
585.700998	29043.104469	31.564736
586.530821	29081.092402	31.569754
586.764480	29124.208676	31.574772
587.108146	29169.208042	31.579789
588.160681	29204.426664	31.584807
588.584549	29253.409899	31.589824
589.013671	29288.283592	31.594842
590.077134	29350.032316	31.599860
590.389052	29400.084937	31.604877
591.280643	29429.429550	31.609895
591.261674	29472.676808	31.614912
592.352964	29523.053241	31.619930
592.992434	29564.066835	31.624948
593.414887	29606.607482	31.629965
594.183367	29641.643787	31.634983
594.492193	29689.015586	31.640000
594.986171	29729.011085	31.645018
595.735949	29769.019527	31.650036
596.222279	29827.992220	31.655053
596.933579	29858.639676	31.660071
597.283420	29906.631222	31.665088
598.238278	29952.162639	31.670106
598.532159	29995.123490	31.675124
599.019537	30038.991330	31.680141
599.864625	30083.516229	31.685159
600.474931	30128.170046	31.690176
601.273005	30178.727590	31.695194
602.106725	30191.279867	31.700212
602.505650	30231.372113	31.705229
602.986142	30262.317123	31.710247
603.402804	30309.993475	31.715264
604.052644	30330.459764	31.720282
604.364587	30368.225868	31.725300
604.885786	30422.410473	31.730317
605.720704	30452.872309	31.735335
606.368832	30507.943180	31.740352
606.831463	30562.282568	31.745370
607.812468	30592.918402	31.750388
608.298573	30640.001536	31.755405
609.078358	30665.430896	31.760423
609.267323	30732.034833	31.765440
610.143192	30762.022649	31.770458
610.796312	30803.413861	31.775476
610.964213	30853.944622	31.780493
611.714675	30881.987320	31.785511
612.101845	30936.246983	31.790528
612.700458	30982.712716	31.795546
613.618066	31030.714861	31.800564
614.108572	31082.241446	31.805581
614.847470	31130.295984	31.810599
615.222553	31185.655333	31.815616
616.228295	31228.135687	31.820634
616.926385	31272.816481	31.825652
617.236907	31326.323671	31.830669
618.117755	31361.158230	31.835687
618.682296	31412.527488	31.840704
618.973783	31472.730240	31.845722
619.934393	31512.260200	31.850740
620.118474	31564.141283	31.855757
621.057020	31605.117111	31.860775
621.657097	31658.046549	31.865792
622.736329	31698.789010	31.870810
623.223389	31744.514984	31.875828
623.812963	31801.066894	31.880845
624.501928	31837.485505	31.885863
624.998629	31888.305955	31.890880
625.657162	31930.230311	31.895898
626.511717	31977.915864	31.900916
626.832835	32030.176934	31.905933
627.929971	32061.090198	31.910951
628.163946	32112.470156	31.915968
628.512447	32150.324386	31.920986
629.303155	32197.547898	31.926004
630.214207	32240.901816	31.931021
630.826195	32294.312137	31.936039
631.211591	32332.893831	31.941056
631.810652	32381.283234	31.946074
632.485094	32428.696153	31.951092
632.966829	32481.319242	31.956109
634.054233	32517.212514	31.961127
634.413145	32568.859290	31.966144
634.840476	32607.920418	31.971162
635.632443	32643.451201	31.976180
636.000883	32697.899351	31.981197
637.101081	32731.678938	31.986215
637.210885	32777.986433	31.991232
637.551530	32827.783301	31.996250
638.461647	32855.413057	32.001268
639.031279	32918.904210	32.006285
639.640794	32965.052267	32.011303
640.355173	33009.870750	32.016320
640.926430	33053.682861	32.021338
641.483586	33101.631824	32.026356
642.120442	33159.300005	32.031373
642.708585	33204.618299	32.036391
643.274603	33263.770346	32.041408
643.765946	33314.211441	32.046426
644.814411	33362.470688	32.051444
645.386054	33420.500096	32.056461
645.947875	33468.797739	32.061479
646.448207	33526.559873	32.066496
647.365040	33572.422673	32.071514
648.263387	33631.534152	32.076532
648.683207	33690.666869	32.081549
649.721287	33732.566902	32.086567
650.154428	33782.602548	32.091584
650.455941	33836.354187	32.096602
651.405255	33892.135609	32.101620
652.106672	33953.004089	32.106637
652.833783	33988.488199	32.111655
653.414170	34049.330591	32.116672
653.906605	34095.716406	32.121690
654.687180	34158.540308	32.126708
655.313440	34208.978409	32.131725
656.015256	34244.656258	32.136743
657.015574	34303.240007	32.141760
657.521414	34377.347931	32.146778
658.703911	34408.590942	32.151796
658.900215	34453.131690	32.156813
659.545298	34499.703986	32.161831
659.977258	34565.126060	32.166848
660.481981	34601.553316	32.171866
661.765189	34646.440145	32.176884
662.122195	34704.795129	32.181901
663.105338	34757.466999	32.186919
663.659420	34796.684938	32.191936
664.053748	34856.361845	32.196954
664.787568	34897.791484	32.201972
665.432750	34966.422295	32.206989
666.233375	35022.368345	32.212007
666.818483	35066.306533	32.217024
667.147354	35121.762094	32.222042
668.201272	35163.288036	32.227060
668.465406	35225.733155	32.232077
669.253197	35280.225478	32.237095
669.913224	35331.325294	32.242112
670.267921	35375.980440	32.247130
671.344104	35414.590166	32.252148
671.725663	35469.031131	32.257165
672.244304	35518.914929	32.262183
672.932402	35574.291149	32.267200
673.611064	35625.502406	32.272218
674.894072	35663.509091	32.277236
675.234215	35717.925932	32.282253
675.590433	35761.533500	32.287271
676.644186	35804.647027	32.292288
676.920410	35857.422326	32.297306
677.636394	35919.835930	32.302324
678.165200	35976.520551	32.307341
678.824767	36030.851291	32.312359
679.804170	36088.159791	32.317376
680.202211	36157.068175	32.322394
681.178464	36210.546619	32.327412
682.130741	36272.045782	32.332429
682.597480	36323.067474	32.337447
683.344479	36371.783920	32.342464
684.270427	36423.948327	32.347482
684.922668	36483.273091	32.352500
685.286843	36541.956545	32.357517
686.065808	36595.209075	32.362535
687.027428	36646.302731	32.367552
687.449069	36712.737563	32.372570
688.442388	36757.684133	32.377588
688.909894	36814.969420	32.382605
689.366407	36865.518259	32.387623
690.392718	36923.298286	32.392640
691.247680	36975.969194	32.397658
691.775237	37018.628859	32.402676
692.335264	37079.819784	32.407693
693.059622	37135.840236	32.412711
694.092111	37184.305474	32.417728
694.447653	37253.649240	32.422746
695.483162	37297.556267	32.427764
696.163402	37367.499958	32.432781
696.425119	37420.161078	32.437799
697.246592	37484.231810	32.442816
698.033484	37537.903884	32.447834
698.771650	37574.286263	32.452852
699.290913	37645.570102	32.457869
700.038678	37711.750412	32.462887
700.853573	37762.427782	32.467904
701.306909	37820.321042	32.472922
701.827412	37879.892447	32.477940
702.733280	37936.829532	32.482957
703.499107	37999.074225	32.487975
704.217064	38059.967644	32.492992
704.903808	38115.205835	32.498010
705.802808	38170.268508	32.503028
706.206476	38232.019869	32.508045
707.260179	38279.296035	32.513063
708.039172	38324.098022	32.518080
708.406010	38376.392201	32.523098
709.056742	38424.653750	32.528116
709.908509	38476.204068	32.533133
710.546505	38531.457689	32.538151
711.418339	38580.945889	32.543168
711.686792	38639.464254	32.548186
712.673333	38693.742083	32.553204
713.154219	38750.602936	32.558221
713.526097	38797.749439	32.563239
714.620451	38854.957625	32.568256
715.032220	38918.028393	32.573274
715.943860	38968.829589	32.578292
716.461892	39040.862180	32.583309
716.966189	39101.687723	32.588327
717.823371	39161.128046	32.593344
718.630002	39224.502910	32.598362
719.670471	39275.979896	32.603380
720.348291	39359.650607	32.608397
721.086096	39412.790873	32.613415
721.903863	39460.557309	32.618432
722.186022	39537.760607	32.623450
722.839554	39592.975796	32.628468
723.644440	39661.508886	32.633485
724.592797	39728.213899	32.638503
725.274498	39790.033896	32.643520
725.769475	39852.721169	32.648538
727.010336	39924.599854	32.653556
727.356784	39986.939122	32.658573
727.800567	40052.071576	32.663591
729.376775	40107.333925	32.668608
729.911363	40180.237582	32.673626
730.878149	40230.179095	32.678644
731.668620	40289.840567	32.683661
731.965169	40357.596391	32.688679
733.198661	40418.562864	32.693696
733.607459	40475.147655	32.698714
734.634525	40529.875915	32.703732
735.284743	40597.603196	32.708749
735.704350	40657.530000	32.713767
736.916223	40706.963963	32.718784
737.227572	40773.257240	32.723802
738.330502	40841.194117	32.728820
738.983390	40879.038532	32.733837
739.486916	40949.799429	32.738855
740.342588	41015.461356	32.743872
740.824866	41092.556250	32.748890
741.843119	41149.642354	32.753908
742.706410	41213.638519	32.758925
743.331784	41273.496876	32.763943
744.261951	41339.659140	32.768960
744.785680	41402.016351	32.773978
745.355906	41457.985736	32.778996
746.169638	41513.342498	32.784013
746.809289	41589.783764	32.789031
747.822630	41635.908704	32.794048
748.422049	41694.479489	32.799066
749.068778	41745.432082	32.804084
749.749828	41809.680275	32.809101
750.363782	41872.113148	32.814119
751.396496	41916.031023	32.819136
752.038944	41987.045344	32.824154
753.104960	42033.500465	32.829172
753.445082	42080.903969	32.834189
753.948261	42157.211779	32.839207
755.025445	42215.105836	32.844224
755.710410	42267.312416	32.849242
756.422691	42333.576287	32.854260
757.019690	42397.111435	32.859277
757.228921	42465.446211	32.864295
758.353529	42522.983637	32.869312
759.198560	42606.200447	32.874330
759.940618	42676.659226	32.879348
761.154753	42742.734383	32.884365
761.521023	42808.462158	32.889383
762.388866	42864.540155	32.894400
762.999081	42940.127829	32.899418
763.707395	43013.700368	32.904436
764.527510	43071.890581	32.909453
764.939329	43162.257399	32.914471
766.248805	43226.871384	32.919488
767.141196	43296.321444	32.924506
767.887595	43372.599071	32.929524
768.682548	43424.599232	32.934541
769.057669	43497.898814	32.939559
770.423720	43565.571167	32.944576
770.849100	43639.118857	32.949594
771.950954	43711.606526	32.954612
772.733368	43775.252875	32.959629
773.221589	43844.778940	32.964647
774.319223	43906.441892	32.969664
774.875366	43980.263584	32.974682
775.620652	44049.673842	32.979700
776.479876	44112.801327	32.984717
776.868481	44189.120581	32.989735
778.087920	44253.572933	32.994752
778.754889	44329.545655	32.999770
779.556278	44400.241764	33.004788
780.746764	44464.242094	33.009805
781.246396	44538.709232	33.014823
781.744924	44603.763453	33.019840
782.669722	44663.715260	33.024858
782.924160	44753.585443	33.029876
784.386748	44812.001016	33.034893
785.300451	44891.258783	33.039911
786.109285	44947.043768	33.044928
786.669050	45024.087103	33.049946
787.256442	45098.709868	33.054964
788.691523	45164.374239	33.059981
788.971081	45230.992549	33.064999
789.890092	45292.401782	33.070016
790.829262	45346.690879	33.075034
791.395565	45397.843713	33.080052
792.519130	45459.896099	33.085069
792.943551	45528.858575	33.090087
793.566167	45585.896155	33.095104
794.508045	45644.750755	33.100122
795.153453	45707.933843	33.105140
796.201385	45758.932204	33.110157
796.824933	45830.602573	33.115175
797.652036	45887.166911	33.120192
798.409438	45954.453312	33.125210
799.162256	46020.065460	33.130228
799.941908	46094.324307	33.135245
800.665777	46169.305358	33.140263
801.659273	46222.746176	33.145280
802.343232	46302.753630	33.150298
802.980438	46378.427683	33.155316
803.795459	46433.642240	33.160333
804.737599	46508.239801	33.165351
805.470055	46576.415958	33.170368
806.032004	46649.058599	33.175386
807.066398	46739.193443	33.180404
807.862529	46804.583941	33.185421
808.600261	46886.980166	33.190439
809.262040	46958.750028	33.195456
810.037718	47039.128004	33.200474
811.109993	47112.593684	33.205492
811.746328	47178.566304	33.210509
812.322943	47263.542409	33.215527
813.268942	47337.322553	33.220544
814.305736	47416.521696	33.225562
814.865093	47501.782504	33.230580
815.654655	47574.736654	33.235597
816.634497	47665.071086	33.240615
817.646907	47743.048215	33.245632
818.701731	47818.403273	33.250650
819.232070	47893.428799	33.255668
820.372812	47958.188178	33.260685
821.327671	48040.826597	33.265703
822.059127	48105.740009	33.270720
823.009297	48180.712557	33.275738
823.572399	48250.499793	33.280756
824.576929	48326.328854	33.285773
825.228713	48402.283803	33.290791
825.877323	48480.587143	33.295808
827.025119	48552.623762	33.300826
827.725712	48629.221915	33.305844
828.906467	48695.107248	33.310861
829.672428	48777.457332	33.315879
830.329712	48857.445931	33.320896
831.513673	48909.883284	33.325914
832.179305	48985.251625	33.330932
833.175103	49057.159878	33.335949
833.531982	49129.450946	33.340967
834.479782	49189.657544	33.345984
835.437301	49258.571874	33.351002
836.122502	49330.211967	33.356020
837.056358	49382.605331	33.361037
837.538561	49453.025501	33.366055
838.172468	49509.329306	33.371072
839.403602	49576.080822	33.376090
839.862117	49650.970606	33.381108
840.649280	49730.273496	33.386125
841.394867	49799.842145	33.391143
842.080135	49880.061253	33.396160
843.163550	49949.400009	33.401178
843.571010	50032.630269	33.406196
844.489095	50104.690825	33.411213
845.314148	50193.819484	33.416231
846.108813	50281.533385	33.421248
847.229854	50364.806253	33.426266
848.072345	50441.102472	33.431284
848.925666	50515.794206	33.436301
849.694698	50605.397724	33.441319
850.675345	50691.847008	33.446336
851.567692	50751.203056	33.451354
852.314975	50852.209760	33.456372
853.375168	50929.745185	33.461389
854.440775	51027.448631	33.466407
855.278200	51099.784818	33.471424
856.482222	51177.667656	33.476442
857.208377	51252.783497	33.481460
858.202425	51320.870017	33.486477
858.617851	51401.359813	33.491495
859.610756	51482.291404	33.496512
860.607012	51557.542265	33.501530
861.468502	51633.553366	33.506548
862.658733	51708.994904	33.511565
863.424404	51788.411342	33.516583
864.062667	51864.212785	33.521600
865.298703	51935.024560	33.526618
865.975250	52018.801923	33.531636
867.044406	52092.799985	33.536653
867.266331	52184.155347	33.541671
868.351816	52261.790349	33.546688
869.480492	52335.035122	33.551706
869.958336	52425.208505	33.556724
870.847124	52501.884857	33.561741
872.208422	52572.287863	33.566759
872.812151	52652.393502	33.571776
874.014280	52729.702668	33.576794
874.618835	52814.120090	33.581812
875.468835	52886.726588	33.586829
876.291617	52967.287961	33.591847
877.053852	53037.860715	33.596864
878.377892	53114.258946	33.601882
878.973246	53210.183820	33.606900
880.250644	53280.827037	33.611917
880.948161	53339.742916	33.616935
881.938250	53425.215973	33.621952
882.639034	53487.212259	33.626970
883.165716	53560.816625	33.631988
883.990402	53623.156624	33.637005
884.622392	53701.845272	33.642023
885.591940	53780.875075	33.647040
886.738413	53842.192495	33.652058
887.368521	53918.205867	33.657076
888.392155	53995.479421	33.662093
889.287465	54077.274621	33.667111
889.653611	54153.675023	33.672128
890.701384	54228.935154	33.677146
891.486004	54313.826460	33.682164
892.521662	54400.067015	33.687181
893.790494	54489.449347	33.692199
894.238626	54568.679188	33.697216
895.439504	54646.968922	33.702234
896.181867	54740.432279	33.707252
897.403461	54816.961321	33.712269
898.353780	54898.145427	33.717287
898.885801	54983.499864	33.722304
899.865271	55068.016472	33.727322
900.694457	55149.609223	33.732340
901.497494	55238.763180	33.737357
902.318729	55331.803516	33.742375
903.275450	55416.912476	33.747392
904.531531	55498.031659	33.752410
904.851225	55596.168916	33.757428
906.142357	55690.809290	33.762445
907.172865	55775.791387	33.767463
908.141726	55860.449088	33.772480
909.171277	55940.738217	33.777498
909.781239	56030.804305	33.782516
910.508866	56128.847937	33.787533
911.852740	56222.608276	33.792551
912.562129	56308.215303	33.797568
914.027718	56382.265650	33.802586
914.652437	56487.632195	33.807604
915.583059	56555.691677	33.812621
916.590871	56634.475230	33.817639
917.102666	56729.014541	33.822656
918.168355	56819.425519	33.827674
919.379172	56912.613929	33.832692
920.275013	56992.717437	33.837709
921.146669	57079.871176	33.842727
922.104065	57166.033065	33.847744
923.143456	57242.077219	33.852762
924.143117	57330.837558	33.857780
924.794055	57422.466598	33.862797
926.013009	57510.826712	33.867815
926.729277	57589.840694	33.872832
927.720842	57676.725624	33.877850
928.662282	57759.385481	33.882868
929.489147	57844.794706	33.887885
930.547629	57927.783959	33.892903
931.461158	58008.353143	33.897920
932.245578	58072.978291	33.902938
933.329975	58148.813821	33.907956
934.265571	58218.804438	33.912973
935.410024	58296.815679	33.917991
935.824490	58366.233111	33.923008
936.886611	58446.875276	33.928026
937.606310	58539.910121	33.933044
938.405235	58614.694323	33.938061
939.498012	58692.102978	33.943079
939.977226	58789.281570	33.948096
941.450759	58870.905126	33.953114
942.064314	58958.866510	33.958132
942.432795	59054.195076	33.963149
943.850289	59143.042863	33.968167
944.355078	59237.896049	33.973184
945.560106	59327.908803	33.978202
946.323726	59427.271309	33.983220
947.359464	59523.967380	33.988237
948.511542	59605.417993	33.993255
949.304398	59707.397864	33.998272
950.684445	59813.004154	34.003290
951.455084	59907.951058	34.008308
952.645946	59997.940891	34.013325
953.787619	60091.528879	34.018343
954.430472	60200.591964	34.023360
955.133055	60286.407920	34.028378
956.213027	60384.061255	34.033396
957.404313	60477.797997	34.038413
958.311945	60570.693106	34.043431
959.220984	60672.571354	34.048448
960.645332	60750.093688	34.053466
961.445834	60849.249502	34.058484
961.969992	60954.976324	34.063501
963.256577	61039.525075	34.068519
964.257451	61145.458141	34.073536
965.524896	61243.616596	34.078554
966.183350	61341.480922	34.083572
967.083065	61427.962246	34.088589
968.424519	61512.134965	34.093607
969.233950	61620.671438	34.098624
969.752514	61721.970203	34.103642
970.935894	61818.013648	34.108660
972.001021	61918.010822	34.113677
972.906600	62011.715433	34.118695
974.130674	62105.382468	34.123712
975.011611	62198.807739	34.128730
976.205829	62295.167663	34.133748
977.124886	62384.542767	34.138765
977.992150	62483.908145	34.143783
978.526100	62585.404878	34.148800
979.959548	62679.710900	34.153818
981.004488	62782.646283	34.158836
981.819548	62867.357217	34.163853
983.038724	62967.963851	34.168871
983.940110	63052.102943	34.173888
985.179504	63134.448660	34.178906
985.618366	63221.475733	34.183924
986.625146	63303.316041	34.188941
987.490606	63378.983407	34.193959
988.204565	63491.673180	34.198976
989.157807	63568.268393	34.203994
990.171712	63665.892421	34.209012
990.872018	63768.436404	34.214029
991.972651	63860.568588	34.219047
992.799427	63965.285143	34.224064
993.962604	64058.952592	34.229082
995.307597	64163.508845	34.234100
996.343772	64252.154097	34.239117
997.716007	64353.738512	34.244135
998.205069	64455.498710	34.249152
999.439047	64542.566394	34.254170
1000.501458	64642.120461	34.259188
1001.481758	64742.048135	34.264205
1002.446503	64834.080324	34.269223
1003.186145	64937.619152	34.274240
1004.355568	65031.230385	34.279258
1005.008734	65131.881671	34.284276
1005.971457	65251.092332	34.289293
1007.215249	65337.603081	34.294311
1007.938267	65458.969173	34.299328
1008.984496	65567.724250	34.304346
1010.230666	65668.577735	34.309364
1010.995313	65779.978065	34.314381
1012.411811	65884.491308	34.319399
1013.369737	65989.457071	34.324416
1014.381712	66098.337463	34.329434
1015.477844	66208.721094	34.334452
1016.622654	66321.286369	34.339469
1017.902520	66407.003454	34.344487
1019.005314	66512.280656	34.349504
1019.891890	66619.263636	34.354522
1021.105813	66718.529603	34.359540
1022.184640	66812.634549	34.364557
1023.372453	66907.051098	34.369575
1023.959069	67009.933735	34.374592
1025.372595	67106.213603	34.379610
1026.223643	67212.160059	34.384628
1026.975155	67317.693368	34.389645
1028.390498	67403.248043	34.394663
1029.503007	67506.911951	34.399680
1030.392317	67616.044686	34.404698
1031.587147	67702.419093	34.409716
1032.173477	67808.884716	34.414733
1033.342541	67913.337775	34.419751
1034.409333	68018.433079	34.424768
1035.383244	68104.383259	34.429786
1036.541597	68209.060722	34.434804
1037.139094	68326.424860	34.439821
1038.584540	68415.314809	34.444839
1039.307754	68505.810973	34.449856
1040.346278	68607.515169	34.454874
1041.721424	68696.790322	34.459892
1041.980698	68783.994342	34.464909
1042.945170	68879.400507	34.469927
1044.257657	68991.423964	34.474944
1045.083021	69080.927321	34.479962
1046.457389	69175.783278	34.484980
1047.425378	69283.200767	34.489997
1048.687029	69382.182170	34.495015
1049.640020	69475.306056	34.500032
1050.406434	69575.156936	34.505050
1051.315996	69692.119536	34.510068
1052.423105	69800.579137	34.515085
1053.587643	69896.748186	34.520103
1054.615546	70012.878869	34.525120
1055.641117	70121.441668	34.530138
1056.545667	70223.832665	34.535156
1057.239202	70345.262454	34.540173
1058.978217	70449.082451	34.545191
1059.964077	70562.916977	34.550208
1060.563254	70671.746506	34.555226
1061.879562	70785.062212	34.560244
1062.779457	70900.750961	34.565261
1064.235108	71012.914852	34.570279
1065.240829	71130.066590	34.575296
1066.354165	71239.164978	34.580314
1067.580413	71345.156326	34.585332
1068.405913	71471.127615	34.590349
1069.505463	71590.042635	34.595367
1070.776753	71695.144116	34.600384
1071.897798	71804.370772	34.605402
1072.978658	71921.395203	34.610420
1074.203102	72043.806206	34.615437
1074.948647	72142.169605	34.620455
1076.321426	72255.377359	34.625472
1077.477269	72363.830693	34.630490
1078.831581	72470.477488	34.635508
1079.689633	72591.711682	34.640525
1081.292634	72688.418585	34.645543
1082.219514	72797.409892	34.650560
1083.010140	72905.974829	34.655578
1084.011216	73013.729661	34.660596
1084.849112	73116.771827	34.665613
1086.480728	73230.746483	34.670631
1087.282856	73351.570832	34.675648
1088.182999	73456.677492	34.680666
1089.814869	73566.628800	34.685684
1090.696560	73681.192923	34.690701
1091.619584	73782.550426	34.695719
1092.573443	73902.045911	34.700736
1093.705910	74023.302044	34.705754
1095.226170	74121.507772	34.710772
1095.812750	74233.644851	34.715789
1097.101768	74338.239310	34.720807
1098.112447	74453.855310	34.725824
1098.879284	74550.451471	34.730842
1100.214014	74648.215340	34.735860
1100.979706	74754.595132	34.740877
1102.187855	74861.360119	34.745895
1103.380967	74958.806774	34.750912
1104.227911	75069.965508	34.755930
1105.297728	75168.336486	34.760948
1106.405902	75293.225284	34.765965
1107.499657	75400.447383	34.770983
1108.638285	75519.373306	34.776000
1109.734324	75634.900369	34.781018
1111.463922	75748.545158	34.786036
1112.109333	75859.999415	34.791053
1113.020270	75978.066844	34.796071
1114.201211	76087.320038	34.801088
1114.992197	76203.695177	34.806106
1116.492796	76320.349964	34.811124
1117.683154	76440.714035	34.816141
1118.694656	76551.639881	34.821159
1120.165282	76688.449779	34.826176
1120.841709	76793.754829	34.831194
1122.158352	76903.224690	34.836212
1122.995501	77029.425026	34.841229
1124.434928	77148.104123	34.846247
1125.391728	77261.071333	34.851264
1126.484510	77392.883562	34.856282
1127.705605	77521.806815	34.861300
1128.610743	77643.898265	34.866317
1129.788003	77770.080706	34.871335
1131.034450	77903.268607	34.876352
1132.070650	78027.604227	34.881370
1133.666134	78151.554595	34.886388
1134.791081	78272.432914	34.891405
1135.583083	78413.426447	34.896423
1136.840126	78528.799000	34.901440
1138.094624	78660.404080	34.906458
1139.248972	78784.371555	34.911476
1140.239699	78912.221455	34.916493
1141.588119	79039.351586	34.921511
1142.891571	79158.026074	34.926528
1143.997775	79285.809371	34.931546
1145.407198	79392.863267	34.936564
1146.421934	79517.160774	34.941581
1147.752832	79644.992744	34.946599
1148.908651	79763.163244	34.951616
1149.835217	79893.197555	34.956634
1151.214219	80003.192433	34.961652
1152.244678	80121.043582	34.966669
1153.407944	80238.501337	34.971687
1154.616006	80370.282776	34.976704
1156.017605	80485.668612	34.981722
1157.279511	80606.968726	34.986740
1157.785277	80724.628621	34.991757
1159.030279	80837.582337	34.996775
1160.511074	80946.131108	35.001792
1161.161996	81058.301830	35.006810
1162.596366	81165.550604	35.011828
1163.462758	81272.599465	35.016845
1164.597728	81385.510451	35.021863
1165.941920	81492.882723	35.026880
1166.765462	81609.277043	35.031898
1168.138595	81722.891614	35.036916
1169.375236	81836.313575	35.041933
1170.182973	81959.388017	35.046951
1171.756249	82069.533664	35.051968
1172.805706	82197.799131	35.056986
1173.893450	82303.294554	35.062004
1175.069402	82426.566071	35.067021
1176.368016	82550.021111	35.072039
1177.482491	82679.334946	35.077056
1178.433948	82807.221458	35.082074
1179.655106	82917.686774	35.087092
1180.494794	83053.640427	35.092109
1181.884769	83182.142274	35.097127
1182.872295	83310.437054	35.102144
1183.842667	83445.575883	35.107162
1185.049165	83579.571655	35.112180
1186.467199	83715.083586	35.117197
1187.549398	83859.450359	35.122215
1188.942857	83990.213640	35.127232
1189.635267	84124.440039	35.132250
1191.286493	84259.633891	35.137268
1192.379721	84400.955238	35.142285
1193.523862	84541.175651	35.147303
1195.084057	84666.650012	35.152320
1196.392741	84817.821943	35.157338
1197.594540	84946.149512	35.162356
1198.777043	85080.860443	35.167373
1200.218718	85207.374799	35.172391
1201.589503	85339.332373	35.177408
1202.539247	85475.669818	35.182426
1203.731296	85604.028211	35.187444
1205.272262	85733.488974	35.192461
1206.255051	85877.290978	35.197479
1207.643617	86001.573901	35.202496
1208.833049	86130.264677	35.207514
1210.120675	86252.371059	35.212532
1211.006640	86388.395698	35.217549
1212.275352	86528.685307	35.222567
1213.543262	86658.467001	35.227584
1214.748228	86796.473226	35.232602
1216.421925	86925.332078	35.237620
1217.616888	87055.045578	35.242637
1218.667827	87186.622825	35.247655
1220.491729	87311.773676	35.252672
1221.245669	87442.704158	35.257690
1222.777512	87559.119811	35.262708
1223.978083	87690.941942	35.267725
1224.813832	87820.982771	35.272743
1226.208964	87926.982186	35.277760
1227.327732	88046.166272	35.282778
1228.357950	88157.334223	35.287796
1229.829344	88267.787600	35.292813
1230.393065	88384.690476	35.297831
1231.797595	88501.276916	35.302848
1232.659214	88618.791353	35.307866
1234.302718	88741.829172	35.312884
1235.644512	88872.542082	35.317901
1236.680609	88990.365956	35.322919
1238.200989	89107.126963	35.327936
1239.476800	89248.223668	35.332954
1240.386722	89366.215096	35.337972
1241.674019	89491.799100	35.342989
1242.602484	89626.857242	35.348007
1244.110599	89746.235436	35.353024
1245.305225	89886.767394	35.358042
1246.542719	90015.543331	35.363060
1247.678428	90153.246872	35.368077
1248.818472	90292.436769	35.373095
1250.260668	90420.290851	35.378112
1251.486726	90552.866291	35.383130
1252.561059	90687.787662	35.388148
1254.051452	90828.019372	35.393165
1255.322181	90978.924447	35.398183
1256.492838	91109.564176	35.403200
1257.998587	91247.626874	35.408218
1259.379361	91374.712079	35.413236
1260.627276	91509.560324	35.418253
1261.425913	91664.687720	35.423271
1263.147654	91780.463391	35.428288
1264.317638	91927.077649	35.433306
1265.589130	92072.044986	35.438324
1267.256319	92206.862478	35.443341
1268.197865	92351.473004	35.448359
1269.636702	92489.092437	35.453376
1271.010046	92618.975243	35.458394
1272.122665	92751.196184	35.463412
1273.517381	92892.651684	35.468429
1274.986517	93035.791340	35.473447
1276.589122	93154.236997	35.478464
1277.804189	93295.211309	35.483482
1278.731555	93433.601035	35.488500
1280.157494	93562.500640	35.493517
1281.390534	93708.458887	35.498535
1282.636056	93822.537297	35.503552
1284.069919	93966.093378	35.508570
1285.526475	94092.612919	35.513588
1286.893211	94238.344659	35.518605
1287.701125	94372.888152	35.523623
1289.325420	94494.595051	35.528640
1290.392000	94631.262252	35.533658
1291.867864	94768.845666	35.538676
1293.188777	94906.176240	35.543693
1294.529120	95031.410212	35.548711
1295.732831	95145.944828	35.553728
1296.671306	95262.767768	35.558746
1297.929004	95389.560319	35.563764
1299.029340	95510.457809	35.568781
1299.862558	95629.057916	35.573799
1301.250002	95775.827467	35.578816
1302.467149	95898.561911	35.583834
1303.796702	96035.967615	35.588852
1304.927644	96173.671414	35.593869
1306.227146	96326.955159	35.598887
1307.253380	96455.694602	35.603904
1308.481274	96616.057724	35.608922
1310.047467	96755.068615	35.613940
1311.793380	96896.487312	35.618957
1312.830927	97048.368935	35.623975
1314.400386	97175.710309	35.628992
1315.733872	97322.821134	35.634010
1316.831961	97475.208411	35.639028
1318.202689	97610.478897	35.644045
1319.343205	97764.816175	35.649063
1320.783072	97897.458307	35.654080
1322.551260	98044.953880	35.659098
1323.628045	98198.779146	35.664116
1325.284854	98348.040470	35.669133
1326.317112	98500.691809	35.674151
1327.588592	98633.054994	35.679168
1328.981269	98792.793619	35.684186
1329.841295	98945.962452	35.689204
1331.611952	99096.722629	35.694221
1333.040516	99249.183110	35.699239
1334.638446	99393.177846	35.704256
1335.785057	99555.225865	35.709274
1337.190533	99704.997846	35.714292
1338.713782	99850.228393	35.719309
1340.102214	100007.312554	35.724327
1341.424119	100128.465123	35.729344
1343.027723	100287.541608	35.734362
1344.424161	100433.808306	35.739380
1345.876838	100578.428290	35.744397
1346.904158	100725.837431	35.749415
1348.414345	100863.812955	35.754432
1349.591636	101015.470908	35.759450
1351.178547	101154.827947	35.764468
1352.716649	101305.664862	35.769485
1353.409976	101457.326700	35.774503
1355.263496	101608.058502	35.779520
1356.747351	101749.574128	35.784538
1357.815580	101898.268671	35.789556
1359.353671	102048.629528	35.794573
1360.998756	102189.774197	35.799591
1362.797145	102334.470402	35.804608
1363.541620	102474.329916	35.809626
1364.392871	102623.234410	35.814644
1366.030511	102762.143755	35.819661
1367.429384	102920.593761	35.824679
1368.793316	103041.647285	35.829696
1370.051240	103177.892208	35.834714
1370.998866	103307.726576	35.839732
1372.690794	103449.928147	35.844749
1373.692523	103599.327475	35.849767
1374.843375	103729.524201	35.854784
1376.427767	103865.145385	35.859802
1377.399753	104016.330234	35.864820
1378.991583	104166.727785	35.869837
1380.031461	104317.827839	35.874855
1381.526399	104470.242388	35.879872
1382.870776	104610.019261	35.884890
1384.449765	104775.028051	35.889908
1385.681146	104927.595013	35.894925
1387.106770	105093.522673	35.899943
1388.443669	105252.770253	35.904960
1389.890671	105408.641053	35.909978
1391.311728	105556.182522	35.914996
1392.718075	105716.751133	35.920013
1394.253966	105885.350047	35.925031
1395.303549	106042.996847	35.930048
1397.224627	106200.658072	35.935066
1398.090805	106360.747294	35.940084
1399.991269	106528.039748	35.945101
1401.100253	106701.623292	35.950119
1402.703571	106860.465873	35.955136
1404.002933	107019.275538	35.960154
1405.616187	107188.504220	35.965172
1407.102608	107347.488850	35.970189
1408.570694	107503.325656	35.975207
1410.185868	107671.595442	35.980224
1411.718375	107820.272363	35.985242
1412.972705	107996.690196	35.990260
1414.541623	108149.072165	35.995277
1415.993957	108312.195125	36.000295
1417.638550	108470.092402	36.005312
1419.286469	108619.268561	36.010330
1420.099423	108773.565757	36.015348
1421.707847	108929.383131	36.020365
1423.129971	109094.446583	36.025383
1424.529699	109266.223828	36.030400
1426.081957	109418.686050	36.035418
1427.565821	109576.350230	36.040436
1429.065065	109733.031918	36.045453
1430.950531	109890.336825	36.050471
1432.252218	110049.798950	36.055488
1433.779188	110197.377311	36.060506
1435.252451	110352.668262	36.065524
1436.299388	110502.489480	36.070541
1437.716378	110657.012751	36.075559
1439.264518	110805.439594	36.080576
1440.735720	110962.095628	36.085594
1441.876822	111130.325411	36.090612
1443.426714	111282.989519	36.095629
1445.152087	111439.810762	36.100647
1446.616220	111590.566110	36.105664
1447.891500	111721.552183	36.110682
1448.989021	111869.835497	36.115700
1450.393907	111997.093043	36.120717
1451.785219	112150.515673	36.125735
1453.027573	112300.506670	36.130752
1454.711952	112447.801314	36.135770
1455.973055	112599.158455	36.140788
1457.314900	112744.635548	36.145805
1458.757006	112906.068873	36.150823
1459.865480	113065.777436	36.155840
1461.612426	113227.423950	36.160858
1463.065223	113388.219334	36.165876
1464.671160	113547.421468	36.170893
1466.093023	113714.263117	36.175911
1467.404610	113869.829730	36.180928
1468.983426	114044.815031	36.185946
1470.232663	114201.368518	36.190964
1471.637951	114356.258547	36.195981
1473.116543	114548.147144	36.200999
1474.875091	114716.657586	36.206016
1476.708371	114860.555855	36.211034
1477.812218	115036.199630	36.216052
1479.513472	115212.332145	36.221069
1481.421253	115366.724381	36.226087
1482.516631	115534.206095	36.231104
1484.176507	115694.457867	36.236122
1485.676919	115881.395971	36.241140
1487.305548	116040.736898	36.246157
1488.596250	116209.711498	36.251175
1490.116219	116378.251930	36.256192
1491.928477	116540.092947	36.261210
1492.987014	116703.447622	36.266228
1494.760290	116869.899741	36.271245
1496.217302	117060.221644	36.276263
1497.913526	117217.723114	36.281280
1499.593383	117373.417374	36.286298
1501.024694	117549.488678	36.291316
1502.585989	117715.745723	36.296333
1503.821871	117882.530411	36.301351
1505.581487	118037.696849	36.306368
1507.066505	118203.133400	36.311386
1508.327634	118380.060546	36.316404
1510.107921	118546.756715	36.321421
1511.778882	118716.801824	36.326439
1513.125102	118876.407893	36.331456
1514.820107	119051.599121	36.336474
1516.379159	119223.381266	36.341492
1518.307921	119391.458638	36.346509
1519.812399	119551.809888	36.351527
1521.047640	119726.648152	36.356544
1522.579845	119872.306781	36.361562
1523.952449	120031.776466	36.366580
1525.481639	120198.168559	36.371597
1526.752403	120361.411374	36.376615
1528.242692	120503.141601	36.381632
1529.839253	120656.152371	36.386650
1531.301883	120811.958838	36.391668
1532.735054	120958.513116	36.396685
1534.166861	121107.158095	36.401703
1535.790241	121272.326258	36.406720
1537.352366	121420.027783	36.411738
1538.417837	121587.122952	36.416756
1539.777977	121738.480506	36.421773
1541.289023	121907.254681	36.426791
1542.725447	122079.423372	36.431808
1544.523597	122246.456983	36.436826
1545.548730	122422.708113	36.441844
1547.586462	122592.466879	36.446861
1548.842550	122760.945045	36.451879
1550.454156	122922.553761	36.456896
1552.477224	123099.157476	36.461914
1553.507427	123271.550436	36.466932
1555.037535	123454.466332	36.471949
1556.706644	123630.724502	36.476967
1558.044017	123814.408105	36.481984
1560.073423	124002.669460	36.487002
1561.621570	124176.974554	36.492020
1563.377417	124356.453590	36.497037
1564.578844	124536.097897	36.502055
1566.239323	124727.488193	36.507072
1567.946183	124899.467494	36.512090
1569.194984	125098.525690	36.517108
1570.817941	125276.815997	36.522125
1573.019924	125462.412858	36.527143
1574.431735	125641.448451	36.532160
1576.153337	125821.639372	36.537178
1577.713754	126008.659252	36.542196
1579.735248	126187.702947	36.547213
1581.260068	126372.932275	36.552231
1582.682780	126550.477421	36.557248
1584.826104	126719.257499	36.562266
1586.032038	126898.600103	36.567284
1587.596645	127073.883998	36.572301
1589.023101	127252.687201	36.577319
1590.474703	127433.096367	36.582336
1592.356759	127611.069488	36.587354
1593.823208	127811.202403	36.592372
1595.488588	127982.131055	36.597389
1597.257290	128160.847818	36.602407
1598.694994	128343.241378	36.607424
1600.632488	128511.191112	36.612442
1602.200627	128705.588396	36.617460
1603.484243	128879.104229	36.622477
1605.279892	129047.548487	36.627495
1606.810870	129240.055177	36.632512
1608.405830	129412.536763	36.637530
1610.150369	129605.822857	36.642548
1611.863129	129780.327665	36.647565
1613.780998	129952.279904	36.652583
1614.987141	130123.687473	36.657600
1616.468688	130267.256738	36.662618
1617.985826	130450.563707	36.667636
1619.531572	130602.954795	36.672653
1620.986958	130746.556019	36.677671
1622.580576	130930.652142	36.682688
1624.028410	131101.254493	36.687706
1625.440850	131269.076241	36.692724
1627.040841	131462.828902	36.697741
1628.866274	131625.734783	36.702759
1630.060992	131808.481026	36.707776
1631.695036	131987.940574	36.712794
1633.522674	132174.896359	36.717812
1634.905338	132365.674332	36.722829
1637.010310	132538.106825	36.727847
1638.394826	132727.379216	36.732864
1639.994482	132918.797956	36.737882
1641.797493	133115.963295	36.742900
1643.277890	133298.357014	36.747917
1645.127087	133478.957488	36.752935
1646.324352	133670.495868	36.757952
1648.110376	133868.733424	36.762970
1649.855308	134066.003243	36.767988
1651.615821	134263.892808	36.773005
1653.339877	134451.310790	36.778023
1655.044181	134662.491012	36.783040
1656.999902	134841.993463	36.788058
1658.530089	135045.373496	36.793076
1659.971722	135234.704072	36.798093
1661.846173	135426.425363	36.803111
1663.604568	135631.509231	36.808128
1665.637277	135819.875443	36.813146
1667.255134	136026.441632	36.818164
1668.888004	136205.332227	36.823181
1670.559921	136410.701433	36.828199
1672.373218	136610.955599	36.833216
1674.120604	136784.560126	36.838234
1675.586110	136981.425334	36.843252
1677.350995	137176.356198	36.848269
1679.211380	137364.354252	36.853287
1680.612920	137561.448937	36.858304
1682.536538	137760.426227	36.863322
1684.219520	137960.482207	36.868340
1685.950125	138153.562165	36.873357
1688.098617	138346.361592	36.878375
1689.737139	138536.962203	36.883392
1691.543717	138716.803634	36.888410
1693.064150	138907.083218	36.893428
1694.815341	139092.739825	36.898445
1696.584231	139282.640194	36.903463
1698.107144	139465.534674	36.908480
1700.258881	139661.180871	36.913498
1701.898406	139848.646820	36.918516
1703.418743	140028.098070	36.923533
1705.584080	140201.415499	36.928551
1707.030960	140366.889169	36.933568
1708.813140	140530.713659	36.938586
1710.154643	140702.631325	36.943604
1711.454249	140855.520971	36.948621
1713.470823	141013.671149	36.953639
1714.860662	141201.172519	36.958656
1716.474572	141364.445275	36.963674
1718.298749	141544.896573	36.968692
1719.864321	141732.449374	36.973709
1721.363067	141901.509940	36.978727
1722.660384	142084.113965	36.983744
1724.786017	142274.648302	36.988762
1726.074561	142466.254644	36.993780
1728.081248	142663.324843	36.998797
1729.731482	142850.642954	37.003815
1731.257054	143046.271094	37.008832
1732.958939	143252.835955	37.013850
1734.595061	143452.327538	37.018868
1736.323892	143648.548299	37.023885
1738.140704	143847.430719	37.028903
1740.016811	144050.855282	37.033920
1741.975729	144254.851084	37.038938
1743.338837	144456.040256	37.043956
1744.986298	144672.078839	37.048973
1747.487267	144863.697729	37.053991
1749.096907	145073.192036	37.059008
1751.103830	145270.469003	37.064026
1753.036473	145468.608268	37.069044
1754.688594	145680.267411	37.074061
1756.435836	145879.440087	37.079079
1758.181722	146078.842407	37.084096
1759.970028	146281.053280	37.089114
1761.803697	146491.548258	37.094132
1762.961826	146698.222363	37.099149
1765.325050	146894.844546	37.104167
1767.161948	147110.502284	37.109184
1768.773415	147308.311193	37.114202
1771.308779	147512.477570	37.119220
1772.531945	147720.086069	37.124237
1774.504481	147911.059569	37.129255
1776.563572	148114.354705	37.134272
1778.254971	148308.582381	37.139290
1780.368639	148503.783683	37.144308
1781.900254	148712.946934	37.149325
1784.009469	148895.740815	37.154343
1785.380148	149102.320736	37.159360
1787.275421	149299.526480	37.164378
1789.173725	149498.393646	37.169396
1791.276082	149686.175194	37.174413
1793.019208	149888.023169	37.179431
1794.420744	150087.746145	37.184448
1796.272248	150275.723074	37.189466
1798.152006	150476.817743	37.194484
1799.733460	150677.251076	37.199501
1801.759552	150861.628625	37.204519
1803.591705	151047.419872	37.209536
1805.151259	151216.558899	37.214554
1807.287674	151401.581230	37.219572
1808.827153	151575.124494	37.224589
1810.303692	151742.834147	37.229607
1811.970520	151935.249203	37.234624
1813.638193	152109.649724	37.239642
1815.592749	152299.041889	37.244660
1816.553410	152492.079431	37.249677
1819.137850	152678.001375	37.254695
1820.905978	152892.250618	37.259712
1822.357361	153086.494241	37.264730
1824.206223	153280.967507	37.269748
1826.001329	153491.095819	37.274765
1828.033749	153684.540699	37.279783
1829.935292	153894.971630	37.284800
1831.446326	154094.029585	37.289818
1833.415728	154291.786107	37.294836
1835.163874	154505.567101	37.299853
1837.079681	154714.428727	37.304871
1838.806883	154927.721248	37.309888
1840.464994	155144.487512	37.314906
1842.618996	155361.544149	37.319924
1844.242865	155588.652325	37.324941
1846.029435	155790.415316	37.329959
1848.118679	156015.043378	37.334976
1850.316960	156223.603220	37.339994
1852.103229	156439.622004	37.345012
1853.971039	156660.726482	37.350029
1855.789487	156869.071611	37.355047
1857.921845	157093.230776	37.360064
1859.990773	157299.865013	37.365082
1861.758056	157522.499930	37.370100
1863.421288	157742.540686	37.375117
1865.764373	157943.961762	37.380135
1867.677017	158150.879518	37.385152
1869.509888	158373.712398	37.390170
1871.783426	158570.710023	37.395188
1873.240272	158791.766604	37.400205
1875.549973	159008.010061	37.405223
1877.557551	159207.386745	37.410240
1879.423392	159405.341456	37.415258
1881.641644	159616.784504	37.420276
1883.124034	159824.173601	37.425293
1885.203070	160023.581635	37.430311
1887.093807	160226.863053	37.435328
1888.755329	160441.316078	37.440346
1891.146529	160637.038547	37.445364
1892.661818	160839.495400	37.450381
1894.745311	161041.711047	37.455399
1896.878051	161244.554103	37.460416
1898.295191	161447.308992	37.465434
1900.396866	161646.976214	37.470452
1902.159604	161858.111840	37.475469
1904.588656	162039.125308	37.480487
1906.056253	162230.818176	37.485504
1907.507308	162419.635912	37.490522
1909.466302	162597.074431	37.495540
1911.165253	162782.620839	37.500557
1912.859137	162967.179807	37.505575
1914.832663	163161.879074	37.510592
1916.419222	163351.884988	37.515610
1918.532587	163547.350431	37.520628
1920.549310	163741.373800	37.525645
1922.490150	163936.057050	37.530663
1924.386085	164141.021258	37.535680
1926.385176	164348.849180	37.540698
1928.464365	164532.327667	37.545716
1930.083968	164734.066948	37.550733
1932.046481	164937.160700	37.555751
1933.883944	165143.293927	37.560768
1935.826806	165356.983259	37.565786
1937.876633	165555.969999	37.570804
1939.617365	165768.932817	37.575821
1942.104273	165967.801676	37.580839
1943.824682	166188.024854	37.585856
1945.903956	166401.026355	37.590874
1947.984644	166597.642023	37.595892
1949.972347	166817.699671	37.600909
1951.940517	167028.857934	37.605927
1953.896925	167233.639444	37.610944
1955.647851	167450.770444	37.615962
1958.137789	167651.740591	37.620980
1959.760454	167877.405140	37.625997
1962.053966	168073.956721	37.631015
1964.248117	168287.445370	37.636032
1965.895465	168504.433975	37.641050
1968.401171	168709.795892	37.646068
1970.101306	168927.095632	37.651085
1971.802316	169135.644406	37.656103
1974.141448	169336.774262	37.661120
1976.184409	169549.596348	37.666138
1977.896309	169770.996040	37.671156
1980.051454	169981.823960	37.676173
1982.272949	170189.179638	37.681191
1984.337094	170387.517306	37.686208
1986.218625	170598.315906	37.691226
1988.544529	170795.637414	37.696244
1990.323682	171006.809653	37.701261
1992.268447	171219.567732	37.706279
1994.353480	171426.304756	37.711296
1996.585439	171628.135849	37.716314
1998.837676	171827.909791	37.721332
2000.675888	172031.911161	37.726349
2002.625740	172234.094582	37.731367
2004.760282	172431.378609	37.736384
2006.600615	172636.029720	37.741402
2008.746675	172834.620522	37.746420
2010.799066	173043.337462	37.751437
2012.742671	173225.369821	37.756455
2014.769090	173402.011206	37.761472
2016.298182	173586.483185	37.766490
2018.440348	173765.099454	37.771508
2020.245105	173943.097718	37.776525
2022.229823	174120.903304	37.781543
2024.576485	174306.428658	37.786560
2026.580779	174511.900657	37.791578
2028.525170	174685.021364	37.796596
2030.465172	174874.165926	37.801613
2032.424261	175067.405942	37.806631
2034.587145	175242.409968	37.811648
2036.227374	175436.146351	37.816666
2038.618525	175639.875443	37.821684
2040.433820	175832.824765	37.826701
2042.384125	176023.431975	37.831719
2044.404211	176220.334152	37.836736
2046.292070	176433.484265	37.841754
2048.366988	176622.678982	37.846772
2050.197473	176835.129836	37.851789
2052.208830	177044.203807	37.856807
2054.592681	177244.516638	37.861824
2056.557785	177455.338110	37.866842
2058.961198	177665.329903	37.871860
2060.956417	177879.777196	37.876877
2063.172800	178077.113818	37.881895
2065.308604	178285.222774	37.886912
2067.478160	178501.358355	37.891930
2069.747744	178700.389553	37.896948
2071.949743	178913.527938	37.901965
2073.932210	179107.785467	37.906983
2076.211750	179310.573415	37.912000
2078.065176	179515.015865	37.917018
2080.887927	179703.814112	37.922036
2082.904024	179907.687088	37.927053
2085.089688	180116.672619	37.932071
2087.417974	180302.532325	37.937088
2089.440021	180502.524783	37.942106
2091.721207	180692.035031	37.947124
2093.778521	180876.658757	37.952141
2095.909450	181076.750812	37.957159
2097.876447	181260.159789	37.962176
2100.102846	181454.490820	37.967194
2102.461060	181652.049955	37.972212
2104.721156	181834.653592	37.977229
2106.426534	182038.116515	37.982247
2108.476097	182221.148509	37.987264
2110.378480	182413.746200	37.992282
2112.722520	182603.191415	37.997300
2115.162882	182804.853773	38.002317
2116.893609	182993.776239	38.007335
2119.456650	183170.272338	38.012352
2121.352235	183374.662938	38.017370
2123.456697	183560.775137	38.022388
2125.735994	183761.528474	38.027405
2127.612513	183947.018646	38.032423
2129.499741	184110.721289	38.037440
2131.217784	184283.676136	38.042458
2133.398043	184447.942601	38.047476
2135.351859	184616.712085	38.052493
2137.696144	184795.888653	38.057511
2139.748064	184964.275907	38.062528
2141.304078	185156.953165	38.067546
2143.679321	185323.628215	38.072564
2145.843601	185518.646844	38.077581
2147.642248	185714.866341	38.082599
2149.961653	185887.249786	38.087616
2151.840488	186087.823284	38.092634
2153.960881	186282.928300	38.097652
2156.188448	186480.694621	38.102669
2158.341700	186679.044612	38.107687
2160.633920	186863.643348	38.112704
2162.845165	187075.728623	38.117722
2165.357175	187275.496284	38.122740
2167.371762	187474.963018	38.127757
2169.299022	187676.652482	38.132775
2171.491992	187868.707186	38.137792
2173.660475	188090.448156	38.142810
2176.218330	188295.796493	38.147828
2178.399805	188494.860445	38.152845
2180.363447	188700.837791	38.157863
2182.567045	188916.308240	38.162880
2184.495517	189130.833482	38.167898
2187.194786	189343.943049	38.172916
2189.051036	189548.431006	38.177933
2191.242261	189768.551948	38.182951
2193.954562	189971.471954	38.187968
2196.184222	190187.667419	38.192986
2198.137345	190402.524461	38.198004
2200.363102	190604.191828	38.203021
2202.723305	190815.217070	38.208039
2205.166082	191024.516907	38.213056
2207.087275	191249.344966	38.218074
2209.370910	191458.849598	38.223092
2212.022539	191664.578367	38.228109
2213.970468	191883.935391	38.233127
2216.448859	192096.280028	38.238144
2218.733607	192313.694622	38.243162
2220.711489	192521.462895	38.248180
2222.816834	192733.615642	38.253197
2224.741163	192945.379205	38.258215
2227.304834	193160.265851	38.263232
2229.696781	193384.991010	38.268250
2231.655938	193597.716381	38.273268
2233.950559	193813.041960	38.278285
2236.022842	194030.142454	38.283303
2238.555816	194250.762523	38.288320
2240.742863	194476.007377	38.293338
2242.997074	194691.127390	38.298356
2245.261000	194905.294908	38.303373
2247.696053	195113.813776	38.308391
2250.097857	195309.850097	38.313408
2251.805616	195500.844368	38.318426
2253.687305	195687.534623	38.323444
2255.855563	195886.186646	38.328461
2257.660025	196093.400731	38.333479
2259.884731	196280.774893	38.338496
2262.227472	196494.365462	38.343514
2264.074214	196704.951391	38.348532
2266.507567	196912.843269	38.353549
2268.491900	197131.278244	38.358567
2270.810365	197355.715358	38.363584
2272.644387	197579.532181	38.368602
2274.909972	197795.094959	38.373620
2277.595151	198026.800298	38.378637
2279.758097	198269.009988	38.383655
2281.961704	198499.524525	38.388672
2284.448672	198731.391320	38.393690
2286.522628	198961.534957	38.398708
2289.134185	199206.685957	38.403725
2291.283173	199444.790797	38.408743
2293.952695	199682.039898	38.413760
2296.090796	199913.078652	38.418778
2298.418862	200154.267995	38.423796
2301.268139	200387.391892	38.428813
2303.259216	200634.450191	38.433831
2306.046545	200858.129628	38.438848
2308.331089	201101.957552	38.443866
2310.596960	201336.117310	38.448884
2313.297671	201576.581132	38.453901
2315.546217	201801.593789	38.458919
2318.074665	202031.437232	38.463936
2320.093641	202269.663893	38.468954
2322.298893	202501.858033	38.473972
2324.950004	202728.701950	38.478989
2327.038734	202986.709799	38.484007
2329.695394	203215.890426	38.489024
2331.794457	203458.361811	38.494042
2334.055596	203697.203521	38.499060
2336.637148	203940.654055	38.504077
2339.024397	204173.714799	38.509095
2341.803199	204409.608623	38.514112
2343.709607	204656.241170	38.519130
2346.159968	204889.269433	38.524148
2348.888440	205112.492828	38.529165
2350.954136	205356.120015	38.534183
2353.605261	205591.937370	38.539200
2355.841880	205827.364405	38.544218
2357.799442	206065.400866	38.549236
2360.337174	206299.271446	38.554253
2362.408106	206545.847837	38.559271
2364.961532	206788.502361	38.564288
2367.322795	207039.909435	38.569306
2369.434804	207284.286244	38.574324
2371.893905	207526.019339	38.579341
2374.338176	207764.099712	38.584359
2376.556655	207990.144204	38.589376
2378.747268	208207.955098	38.594394
2380.759242	208432.688344	38.599412
2383.240846	208646.265417	38.604429
2385.249783	208891.299817	38.609447
2387.397263	209107.330797	38.614464
2389.831522	209338.576389	38.619482
2391.600416	209586.977692	38.624500
2394.323244	209817.709622	38.629517
2396.659208	210070.225026	38.634535
2398.819387	210333.420541	38.639552
2401.413086	210582.266352	38.644570
2403.250901	210837.517117	38.649588
2406.158912	211093.056299	38.654605
2408.266100	211363.183457	38.659623
2410.941873	211621.452998	38.664640
2412.990328	211882.133597	38.669658
2415.053707	212152.689991	38.674676
2418.217083	212425.320271	38.679693
2420.623430	212705.981067	38.684711
2422.935773	212975.054139	38.689728
2425.691153	213232.327257	38.694746
2428.249422	213518.210799	38.699764
2430.895678	213775.046297	38.704781
2433.286513	214056.489787	38.709799
2435.945599	214323.989915	38.714816
2438.747567	214592.826940	38.719834
2440.623033	214873.593812	38.724852
2443.580336	215132.467393	38.729869
2445.696342	215402.038490	38.734887
2448.311247	215688.201663	38.739904
2450.985434	215952.011277	38.744922
2453.613746	216231.128195	38.749940
2456.060801	216491.687550	38.754957
2458.486736	216769.340557	38.759975
2460.855602	217039.931811	38.764992
2463.938899	217307.668442	38.770010
2465.829100	217586.031740	38.775028
2468.845900	217844.245869	38.780045
2471.229357	218111.118844	38.785063
2473.704838	218379.666893	38.790080
2476.470308	218652.004400	38.795098
2478.756964	218930.335522	38.800116
2481.112069	219188.646695	38.805133
2483.493470	219465.225398	38.810151
2486.023676	219746.707968	38.815168
2488.874833	220008.828690	38.820186
2490.922322	220293.487920	38.825204
2493.570808	220560.759619	38.830221
2496.086327	220829.221486	38.835239
2498.379754	221114.682895	38.840256
2501.133392	221384.531099	38.845274
2503.355713	221664.888900	38.850292
2505.831514	221928.904263	38.855309
2508.128793	222204.427212	38.860327
2510.679190	222457.309729	38.865344
2513.267337	222700.511674	38.870362
2515.298571	222959.839515	38.875380
2517.818363	223258.059399	38.880397
2520.307710	223503.222234	38.885415
2522.771973	223772.731063	38.890432
2525.287161	224030.703306	38.895450
2527.871250	224288.614679	38.900468
2530.063755	224541.814607	38.905485
2532.106548	224822.745534	38.910503
2534.842177	225095.377576	38.915520
2537.554218	225363.252589	38.920538
2540.064966	225643.375735	38.925556
2542.304490	225909.943354	38.930573
2544.992278	226202.941437	38.935591
2547.444624	226488.105106	38.940608
2550.213219	226764.356403	38.945626
2552.310907	227058.771605	38.950644
2554.863323	227351.134870	38.955661
2557.510614	227650.315728	38.960679
2560.047237	227947.407268	38.965696
2563.215048	228248.666438	38.970714
2565.146236	228557.132077	38.975732
2568.416353	228842.834375	38.980749
2570.706049	229148.426263	38.985767
2572.973951	229445.260743	38.990784
2575.797300	229754.300333	38.995802
2578.256197	230059.792362	39.000820
2581.344479	230359.191980	39.005837
2584.003046	230673.975202	39.010855
2586.414003	230966.779281	39.015872
2589.642804	231270.299396	39.020890
2591.881069	231583.196736	39.025908
2594.976542	231883.438317	39.030925
2597.595081	232189.343908	39.035943
2600.110393	232488.079294	39.040960
2603.034573	232782.052247	39.045978
2605.857274	233091.204715	39.050996
2608.308941	233384.797221	39.056013
2611.012489	233677.258593	39.061031
2613.374021	233978.257997	39.066048
2616.299874	234267.028583	39.071066
2619.028748	234577.597526	39.076084
2621.592509	234873.538757	39.081101
2624.315039	235161.404410	39.086119
2626.682813	235473.938214	39.091136
2629.429926	235771.580119	39.096154
2631.839887	236065.949080	39.101172
2634.456288	236368.743940	39.106189
2636.985056	236670.690003	39.111207
2639.356978	236973.550742	39.116224
2642.252708	237283.237868	39.121242
2644.890473	237592.103195	39.126260
2647.468451	237899.785122	39.131277
2650.262884	238195.140449	39.136295
2652.711169	238475.159494	39.141312
2655.402023	238751.407131	39.146330
2657.897691	239023.520888	39.151348
2660.380017	239293.427674	39.156365
2662.620715	239585.801096	39.161383
2664.939626	239875.343533	39.166400
2667.631271	240160.154132	39.171418
2670.188548	240471.148351	39.176436
2672.408510	240762.080264	39.181453
2675.163897	241069.920525	39.186471
2677.906450	241373.547246	39.191488
2680.651048	241686.038980	39.196506
2682.912704	242007.828213	39.201524
2685.371119	242327.199522	39.206541
2688.008380	242650.683546	39.211559
2690.364007	242986.557505	39.216576
2693.257522	243319.476929	39.221594
2696.185826	243655.414352	39.226612
2698.643635	243999.225097	39.231629
2702.024070	244333.543245	39.236647
2704.427558	244674.189318	39.241664
2707.085993	245008.699747	39.246682
2709.809957	245359.660237	39.251700
2712.723417	245699.288311	39.256717
2715.757567	246037.450266	39.261735
2718.512434	246390.008745	39.266752
2721.782954	246722.851552	39.271770
2724.356872	247065.305428	39.276788
2727.038077	247409.089379	39.281805
2729.867421	247747.338648	39.286823
2732.630136	248093.473593	39.291840
2735.526725	248443.195104	39.296858
2738.598734	248786.717140	39.301876
2741.212348	249119.567807	39.306893
2744.072442	249456.723778	39.311911
2746.873233	249813.169527	39.316928
2749.902539	250149.893754	39.321946
2752.711419	250488.025278	39.326964
2755.398955	250831.257030	39.331981
2758.582173	251162.091208	39.336999
2761.559077	251499.207521	39.342016
2764.152467	251834.022882	39.347034
2766.378736	252164.807352	39.352052
2769.451003	252501.554893	39.357069
2772.318546	252845.270200	39.362087
2774.670762	253188.712148	39.367104
2777.582753	253531.558047	39.372122
2780.367711	253881.842077	39.377140
2783.087311	254211.155023	39.382157
2786.325095	254552.300044	39.387175
2789.144891	254897.627002	39.392192
2792.159516	255239.342000	39.397210
2794.428773	255590.193402	39.402228
2797.411842	255920.483545	39.407245
2800.537440	256250.116582	39.412263
2802.567612	256571.845664	39.417280
2805.368302	256865.967845	39.422298
2807.978459	257173.609266	39.427316
2810.531033	257490.379703	39.432333
2813.164800	257808.077615	39.437351
2815.712021	258133.740651	39.442368
2818.152378	258456.855403	39.447386
2820.881593	258795.344208	39.452404
2823.472730	259136.039969	39.457421
2826.400676	259475.793765	39.462439
2829.156943	259827.997107	39.467456
2831.972980	260176.076220	39.472474
2834.560582	260521.219837	39.477492
2837.228379	260890.102783	39.482509
2839.852583	261243.776835	39.487527
2842.942688	261616.861523	39.492544
2845.767728	261981.173859	39.497562
2848.188762	262370.115206	39.502580
2851.245383	262742.927147	39.507597
2854.727330	263104.723497	39.512615
2857.578624	263499.745595	39.517632
2860.763139	263875.002647	39.522650
2863.464502	264243.935033	39.527668
2866.344003	264623.432664	39.532685
2869.470370	265003.882308	39.537703
2872.142253	265380.212769	39.542720
2875.213878	265752.441185	39.547738
2878.357063	266137.156954	39.552756
2881.111567	266530.673294	39.557773
2884.350443	266907.702812	39.562791
2887.032884	267294.804192	39.567808
2890.117458	267667.362354	39.572826
2893.175376	268049.120979	39.577844
2895.905737	268439.645050	39.582861
2899.051074	268814.988723	39.587879
2902.049695	269203.032102	39.592896
2905.353541	269578.833793	39.597914
2907.920194	269964.253246	39.602932
2910.966345	270333.186421	39.607949
2914.066464	270711.866111	39.612967
2916.769419	271097.645576	39.617984
2919.598182	271493.871471	39.623002
2922.881359	271869.118590	39.628020
2925.747976	272248.267691	39.633037
2928.969874	272636.455074	39.638055
2931.687341	273019.514720	39.643072
2934.695117	273391.096958	39.648090
2937.617870	273773.260543	39.653108
2940.620731	274156.884904	39.658125
2943.855302	274534.579036	39.663143
2946.256977	274925.055954	39.668160
2949.178950	275298.785878	39.673178
2952.633383	275679.976332	39.678196
2955.307986	276070.511668	39.683213
2958.736343	276440.731941	39.688231
2961.074065	276791.386376	39.693248
2964.101269	277132.075100	39.698266
2966.588397	277482.604177	39.703284
2969.264892	277826.879381	39.708301
2972.426505	278172.779750	39.713319
2974.975888	278547.609797	39.718336
2977.950084	278895.825958	39.723354
2981.000697	279264.911492	39.728372
2983.840375	279627.984285	39.733389
2986.750387	279998.590605	39.738407
2989.231584	280381.331233	39.743424
2992.082769	280759.821568	39.748442
2995.109142	281143.593278	39.753460
2997.837803	281541.917188	39.758477
3001.066886	281934.496717	39.763495
3004.125944	282327.331542	39.768512
3006.985402	282728.250527	39.773530
3009.938390	283128.519339	39.778548
3012.650987	283542.899274	39.783565
3016.130477	283946.970804	39.788583
3019.078978	284368.146158	39.793600
3022.126536	284791.591725	39.798618
3025.388986	285205.349683	39.803636
3027.880831	285627.002542	39.808653
3031.264693	286046.887975	39.813671
3034.718717	286467.752563	39.818688
3037.531299	286903.147096	39.823706
3040.760664	287316.247531	39.828724
3043.943168	287740.938624	39.833741
3047.072465	288155.501832	39.838759
3050.267052	288588.445849	39.843776
3053.528750	289008.194567	39.848794
3056.636269	289421.641800	39.853812
3059.535734	289865.274453	39.858829
3062.756652	290275.095314	39.863847
3065.983260	290725.304929	39.868864
3068.982872	291139.122321	39.873882
3072.305956	291575.648589	39.878900
3075.230030	291998.215037	39.883917
3078.570296	292426.506665	39.888935
3081.582416	292854.417616	39.893952
3084.947628	293272.745999	39.898970
3087.988986	293696.078327	39.903988
3090.969985	294118.200091	39.909005
3094.092031	294537.352053	39.914023
3097.234049	294966.483103	39.919040
3100.310731	295401.313692	39.924058
3103.419810	295829.178049	39.929076
3106.616985	296269.753977	39.934093
3109.917225	296692.226380	39.939111
3112.805857	297126.549485	39.944128
3115.996031	297558.029661	39.949146
3119.286878	297978.798729	39.954164
3122.373940	298416.897661	39.959181
3125.446377	298823.347308	39.964199
3128.097242	299222.801057	39.969216
3131.037219	299617.585038	39.974234
3134.189550	300004.256808	39.979252
3136.593364	300411.468890	39.984269
3139.696272	300802.998279	39.989287
3142.681948	301212.351599	39.994304
3145.619120	301633.218306	39.999322
3148.466911	302048.509752	40.004340
3150.931814	302487.128083	40.009357
3154.540707	302913.422426	40.014375
3157.631751	303353.691813	40.019392
3160.659398	303804.206462	40.024410
3163.771345	304238.119625	40.029428
3166.616581	304694.908918	40.034445
3169.924960	305138.135687	40.039463
3173.309075	305604.107948	40.044480
3176.099015	306065.346519	40.049498
3179.685163	306521.529840	40.054516
3182.769503	306987.316078	40.059533
3186.017633	307454.090730	40.064551
3189.504270	307929.106369	40.069568
3192.860695	308396.419205	40.074586
3196.350162	308876.840981	40.079604
3199.384987	309341.102308	40.084621
3202.801065	309816.299600	40.089639
3205.860137	310282.331406	40.094656
3209.423239	310755.876067	40.099674
3212.963042	311215.935384	40.104692
3215.908392	311704.686500	40.109709
3219.184286	312163.310552	40.114727
3222.547409	312638.606108	40.119744
3225.941653	313124.613044	40.124762
3229.398429	313587.545736	40.129780
3232.666202	314068.412438	40.134797
3236.154565	314530.828042	40.139815
3239.365064	315019.039647	40.144832
3242.786550	315484.534790	40.149850
3246.252316	315948.344511	40.154868
3249.430582	316423.652142	40.159885
3252.643053	316891.815240	40.164903
3256.411701	317365.323281	40.169920
3259.493699	317836.245465	40.174938
3262.626852	318300.071298	40.179956
3265.682832	318767.335743	40.184973
3269.199923	319244.709289	40.189991
3272.869633	319708.798860	40.195008
3275.877779	320179.238434	40.200026
3279.426807	320639.405815	40.205044
3282.796737	321128.145281	40.210061
3285.789566	321586.998944	40.215079
3289.114000	322060.807172	40.220096
3292.111893	322523.515424	40.225114
3295.922872	322988.632228	40.230132
3298.739583	323469.954171	40.235149
3302.283647	323919.768802	40.240167
3305.170322	324358.713958	40.245184
3307.978477	324799.319945	40.250202
3311.247469	325230.555878	40.255220
3314.124199	325661.648413	40.260237
3317.584953	326112.124552	40.265255
3320.516322	326554.834763	40.270272
3323.712976	327006.363447	40.275290
3326.785529	327467.711632	40.280308
3330.042296	327937.662195	40.285325
3333.457562	328404.334327	40.290343
3336.764367	328880.365954	40.295360
3339.883581	329358.785948	40.300378
3343.359906	329831.940628	40.305396
3346.500147	330328.990440	40.310413
3349.731420	330795.626103	40.315431
3353.310886	331293.793471	40.320448
3356.604492	331781.185012	40.325466
3359.634803	332286.390231	40.330484
3362.882254	332803.136817	40.335501
3366.537719	333294.752270	40.340519
3370.161821	333808.918035	40.345536
3373.364281	334315.097238	40.350554
3377.043937	334832.700030	40.355572
3380.461971	335346.709199	40.360589
3383.887364	335855.990403	40.365607
3386.974211	336378.931309	40.370624
3390.490880	336905.354978	40.375642
3394.157614	337415.017790	40.380660
3397.635471	337946.517570	40.385677
3401.144276	338473.996340	40.390695
3404.745214	338996.479637	40.395712
3407.963688	339518.054307	40.400730
3411.756157	340034.633587	40.405748
3415.281354	340564.885418	40.410765
3418.584402	341088.794999	40.415783
3422.356045	341609.757017	40.420800
3425.840202	342134.771626	40.425818
3429.449686	342660.447414	40.430836
3433.040886	343186.959369	40.435853
3436.296051	343697.397914	40.440871
3440.220554	344218.186380	40.445888
3443.519548	344746.711079	40.450906
3447.332834	345252.198779	40.455924
3450.779167	345787.164774	40.460941
3454.014289	346290.322997	40.465959
3457.678511	346810.951741	40.470976
3461.191304	347329.873340	40.475994
3464.822682	347842.120026	40.481012
3468.039971	348352.726598	40.486029
3471.655506	348877.329700	40.491047
3475.446707	349389.257667	40.496064
3478.266302	349910.676569	40.501082
3482.174669	350422.652523	40.506100
3485.543465	350940.116089	40.511117
3488.826232	351444.100083	40.516122
3492.322144	351906.512020	40.521127
3495.129961	352334.442345	40.526132
3498.013777	352697.740432	40.531136
3500.628599	353020.537422	40.536141
3502.790621	353284.412284	40.541146
3504.973484	353526.217978	40.546151
3506.441681	353699.244541	40.551156
3508.934975	353852.792577	40.556160
3510.611455	353958.039687	40.561165
3511.797061	354014.680149	40.566170
3513.040100	354059.961199	40.571175
3513.946653	354078.624824	40.576180
3514.850876	354045.983556	40.581184
3515.431756	354016.599965	40.586189
3515.480505	353957.575950	40.591194
3516.280086	353882.400223	40.596199
3516.411939	353801.476638	40.601204
3516.841180	353703.047755	40.606208
3517.081732	353595.486779	40.611213
3516.911136	353485.521994	40.616218
3516.824648	353350.246995	40.621223
3516.917486	353211.813015	40.626228
3516.586533	353081.309565	40.631232
3516.808348	352942.879935	40.636237
3516.299385	352807.237679	40.641242
3516.218560	352663.383480	40.646247
3515.884170	352534.940646	40.651252
3515.758815	352384.170384	40.656256
3515.864123	352240.082010	40.661261
3515.305606	352114.600327	40.666266
3515.471331	351959.659946	40.671271
3514.872863	351824.741922	40.676276
3514.843657	351685.890586	40.681280
3514.443681	351554.707128	40.686285
3514.085373	351430.362896	40.691290
3514.040752	351289.655095	40.696295
3513.485562	351171.754882	40.701300
3513.259709	351036.470561	40.706304
3512.960236	350921.328928	40.711309
3512.752641	350799.988028	40.716314
3512.522753	350709.903788	40.721319
3512.041070	350602.934490	40.726324
3512.185697	350482.478871	40.731328
3511.979225	350373.938568	40.736333
3511.723432	350274.568155	40.741338
3511.859364	350171.699760	40.746343
3511.437215	350073.500569	40.751348
3511.112737	349974.191368	40.756352
3510.603039	349882.572030	40.761357
3511.043598	349778.942109	40.766362
3510.563132	349694.724101	40.771367
3509.908597	349615.801874	40.776372
3510.263992	349528.371879	40.781376
3509.820729	349446.412766	40.786381
3509.911517	349366.557914	40.791386
3509.744382	349287.303649	40.796391
3509.282043	349219.752656	40.801396
3509.142580	349157.826194	40.806400
3509.184370	349083.501626	40.811405
3508.764250	349022.586535	40.816410
3508.606540	348942.923063	40.821415
3508.642905	348890.054680	40.826420
3508.431934	348821.750821	40.831424
3508.396438	348763.039825	40.836429
3508.212236	348723.517315	40.841434
3508.279411	348651.071570	40.846439
3507.903921	348602.594797	40.851444
3507.764626	348543.569108	40.856448
3508.013937	348501.509095	40.861453
3507.752267	348445.098719	40.866458
3507.858316	348395.069440	40.871463
3507.415711	348351.209820	40.876468
3507.737908	348305.244020	40.881472
3507.325333	348249.926277	40.886477
3507.097721	348206.210718	40.891482
3507.294581	348165.456786	40.896487
3507.364541	348127.242620	40.901492
3506.916248	348080.660339	40.906496
3507.009783	348038.242827	40.911501
3506.898078	348001.711667	40.916506
3506.651511	347963.394717	40.921511
3506.427127	347936.222182	40.926516
3506.906870	347894.227092	40.931520
3506.735867	347863.075578	40.936525
3506.292493	347826.062246	40.941530
3506.544890	347793.189379	40.946535
3506.410332	347770.482114	40.951540
3506.321692	347734.303462	40.956544
3506.286037	347701.679696	40.961549
3506.274648	347671.368212	40.966554
3506.168615	347638.221042	40.971559
3505.870071	347630.123678	40.976564
3506.245028	347601.914505	40.981568
3506.006254	347571.333489	40.986573
3506.126308	347559.962974	40.991578
3506.127286	347532.347383	40.996583
3505.991939	347510.836388	41.001588
3506.141842	347481.975526	41.006592
3506.098552	347451.465350	41.011597
3505.856001	347423.455518	41.016602
3505.975915	347397.170023	41.021607
3505.675256	347365.173357	41.026612
3506.034975	347351.855997	41.031616
3505.845976	347327.171889	41.036621
3505.425636	347306.953030	41.041626
3505.506651	347284.135133	41.046631
3505.601298	347269.027099	41.051636
3505.811295	347251.228339	41.056640
3505.593204	347232.173735	41.061645
3505.401992	347210.213317	41.066650
3505.216504	347196.600329	41.071655
3505.276925	347182.923010	41.076660
3505.702132	347166.820956	41.081664
3505.426068	347143.575860	41.086669
3505.457159	347128.325122	41.091674
3505.837657	347108.106848	41.096679
3505.879442	347091.149105	41.101684
3505.798076	347060.339310	41.106688
3505.627596	347039.113666	41.111693
3505.449721	347021.528868	41.116698
3505.739840	346989.489498	41.121703
3505.462241	346993.784029	41.126708
3505.474510	346954.101953	41.131712
3505.471251	346946.772285	41.136717
3505.400028	346920.135000	41.141722
3505.472960	346893.805794	41.146727
3505.431196	346874.850456	41.151732
3505.355259	346862.289070	41.156736
3505.356293	346849.715513	41.161741
3505.440525	346820.762888	41.166746
3505.363620	346805.885472	41.171751
3505.433200	346794.090092	41.176756
3505.171165	346779.216483	41.181760
3505.180288	346774.557343	41.186765
3504.847267	346749.997563	41.191770
3505.198939	346735.001469	41.196775
3505.156633	346717.496954	41.201780
3505.519148	346709.396761	41.206784
3505.370479	346697.355887	41.211789
3505.347649	346690.054733	41.216794
3505.442057	346665.223723	41.221799
3504.870073	346650.373629	41.226804
3505.298528	346636.281661	41.231808
3505.161209	346608.305696	41.236813
3505.022270	346594.761563	41.241818
3505.134893	346582.043043	41.246823
3505.079330	346568.867511	41.251828
3505.237723	346552.985633	41.256832
3504.952121	346541.042732	41.261837
3505.027237	346524.639508	41.266842
3505.505324	346507.205375	41.271847
3505.157386	346499.573805	41.276852
3505.135078	346475.092048	41.281856
3504.991124	346478.601912	41.286861
3504.710957	346457.164319	41.291866
3505.127645	346437.576400	41.296871
3504.666275	346429.733680	41.301876
3505.016187	346419.293798	41.306880
3504.928872	346403.170744	41.311885
3504.694996	346409.927311	41.316890
3504.818036	346373.230728	41.321895
3504.774960	346372.652228	41.326900
3505.009814	346366.353853	41.331904
3505.320677	346357.090955	41.336909
3504.976792	346342.688320	41.341914
3504.801345	346330.880676	41.346919
3504.924294	346330.250476	41.351924
3505.087644	346298.663456	41.356928
3504.939008	346292.247530	41.361933
3504.561216	346284.467935	41.366938
3504.763783	346272.880497	41.371943
3504.645902	346263.990797	41.376948
3504.738948	346262.652649	41.381952
3505.106641	346251.115460	41.386957
3504.925645	346243.304747	41.391962
3505.050144	346228.980752	41.396967
3504.762328	346217.241755	41.401972
3505.244457	346202.504877	41.406976
3504.949184	346188.196329	41.411981
3504.885097	346181.003443	41.416986
3505.111303	346155.031458	41.421991
3505.048811	346142.900485	41.426996
3504.744105	346130.909613	41.432000
3505.053007	346120.832499	41.437005
3504.831496	346098.138314	41.442010
3505.099395	346090.307519	41.447015
3504.734573	346073.591925	41.452020
3504.978327	346054.438461	41.457024
3504.946621	346047.978570	41.462029
3504.578645	346046.127887	41.467034
3505.090387	346024.972182	41.472039
3505.130568	346011.705027	41.477044
3504.897631	346001.280855	41.482048
3505.013573	345987.314492	41.487053
3504.618997	345970.298139	41.492058
3504.880884	345949.512793	41.497063
3504.512160	345947.534961	41.502068
3504.850628	345938.674877	41.507072
3504.815275	345943.414792	41.512077
3504.312949	345927.662649	41.517082
3504.423541	345904.152300	41.522087
3504.569795	345910.441583	41.527092
3504.709227	345911.310491	41.532096
3504.705490	345895.250440	41.537101
3504.446732	345894.324241	41.542106
3504.598646	345884.475527	41.547111
3504.565756	345881.070146	41.552116
3504.861982	345867.507951	41.557120
3504.821626	345868.481641	41.562125
3504.395779	345851.572008	41.567130
3504.541260	345848.316596	41.572135
3504.459295	345839.217529	41.577140
3504.820469	345807.929853	41.582144
3504.783544	345813.789954	41.587149
3504.653921	345795.586283	41.592154
3505.010960	345784.432479	41.597159
3504.478320	345788.767419	41.602164
3504.643415	345762.728560	41.607168
3504.750938	345769.711210	41.612173
3504.665054	345756.463927	41.617178
3504.875030	345755.081829	41.622183
3504.683982	345747.374449	41.627188
3504.524493	345712.020210	41.632192
3504.497338	345715.053502	41.637197
3504.872544	345712.932599	41.642202
3504.923149	345690.806105	41.647207
3504.597853	345684.799834	41.652212
3504.497527	345665.700638	41.657216
3504.806860	345653.078079	41.662221
3504.874194	345659.812567	41.667226
3504.570154	345639.880167	41.672231
3504.953321	345642.085006	41.677236
3504.826145	345615.761398	41.682240
3504.873885	345618.146531	41.687245
3504.677909	345592.062865	41.692250
3504.769922	345580.314596	41.697255
3504.746420	345574.031526	41.702260
3504.748616	345567.260786	41.707264
3504.925011	345549.314094	41.712269
3504.536855	345549.044670	41.717274
3504.794572	345535.208503	41.722279
3504.722653	345532.318332	41.727284
3504.628458	345512.123636	41.732288
3504.377351	345504.018471	41.737293
3504.585665	345510.196175	41.742298
3504.293760	345481.964120	41.747303
3503.983506	345484.685837	41.752308
3504.457348	345479.978577	41.757312
3504.582566	345491.667273	41.762317
3504.547025	345467.696242	41.767322
3504.640731	345467.248828	41.772327
3504.446876	345458.752809	41.777332
3504.513036	345440.161732	41.782336
3504.776027	345437.244063	41.787341
3504.237174	345445.321608	41.792346
3504.963394	345414.357805	41.797351
3504.566431	345417.347764	41.802356
3504.374642	345405.720686	41.807360
3504.682825	345385.385974	41.812365
3504.119211	345382.446263	41.817370
3504.703057	345380.623254	41.822375
3504.527897	345365.862811	41.827380
3504.432233	345359.871110	41.832384
3504.590063	345361.857053	41.837389
3504.191957	345340.106800	41.842394
3504.603415	345334.111283	41.847399
3504.251187	345329.203716	41.852404
3504.445592	345329.351255	41.857408
3504.399524	345317.548403	41.862413
3504.365664	345304.267339	41.867418
3504.536661	345316.559707	41.872423
3504.420639	345308.636784	41.877428
3504.872915	345284.919448	41.882432
3504.171129	345285.844995	41.887437
3504.042115	345295.715846	41.892442
3504.490377	345272.406389	41.897447
3504.530881	345258.019074	41.902452
3504.160404	345259.961276	41.907456
3504.515734	345258.327108	41.912461
3504.219231	345249.669116	41.917466
3504.224166	345228.033275	41.922471
3504.216065	345239.386754	41.927476
3504.363215	345238.014576	41.932480
3504.499042	345232.368062	41.937485
3504.203210	345220.171973	41.942490
3504.251244	345212.655803	41.947495
3504.360976	345225.746924	41.952500
3504.588138	345209.039305	41.957504
3504.506353	345200.296454	41.962509
3504.600635	345187.631433	41.967514
3504.571439	345181.781925	41.972519
3504.418644	345175.366533	41.977524
3504.760645	345154.848222	41.982528
3504.854649	345152.059067	41.987533
3504.267459	345150.802980	41.992538
3504.316689	345149.039030	41.997543
3504.800890	345143.133806	42.002548
3504.539438	345128.641477	42.007552
3504.590431	345121.684798	42.012557
3504.619884	345110.175403	42.017562
3504.627154	345093.197077	42.022567
3504.405846	345091.628613	42.027572
3504.288942	345086.302025	42.032576
3504.473135	345066.623134	42.037581
3504.110958	345066.705946	42.042586
3504.592024	345053.572498	42.047591
3504.331466	345056.006393	42.052596
3504.365749	345046.634292	42.057600
3504.277804	345038.401454	42.062605
3504.631566	345037.251140	42.067610
3504.836613	345028.208385	42.072615
3504.426160	345019.492012	42.077620
3504.359524	345004.816134	42.082624
3504.695301	344997.508980	42.087629
3504.367969	344992.699261	42.092634
3504.646918	344992.706169	42.097639
3504.536363	344975.237371	42.102644
3504.381400	344956.350205	42.107648
3504.326111	344966.082190	42.112653
3504.501936	344954.040559	42.117658
3504.888776	344938.071217	42.122663
3504.447422	344928.901557	42.127668
3504.573094	344920.991278	42.132672
3504.560005	344899.561791	42.137677
3504.498528	344892.826492	42.142682
3504.563171	344906.790224	42.147687
3504.410386	344882.710221	42.152692
3504.305122	344873.614687	42.157696
3504.549166	344858.431497	42.162701
3504.432490	344854.021170	42.167706
3504.623878	344833.526558	42.172711
3504.549975	344841.836120	42.177716
3504.545960	344833.131826	42.182720
3504.450240	344814.617048	42.187725
3504.405126	344812.715283	42.192730
3504.479724	344812.856311	42.197735
3504.469838	344795.396997	42.202740
3504.268424	344776.924370	42.207744
3504.213128	344777.213200	42.212749
3504.024345	344788.137171	42.217754
3504.101450	344773.133071	42.222759
3504.024197	344755.633489	42.227764
3504.149507	344755.206526	42.232768
3504.431369	344749.536878	42.237773
3504.441832	344767.429023	42.242778
3504.515746	344749.065581	42.247783
3504.282556	344742.179237	42.252788
3504.560840	344731.215857	42.257792
3504.623615	344729.729739	42.262797
3504.145322	344722.322169	42.267802
3504.067951	344713.196746	42.272807
3503.817935	344719.828793	42.277812
3504.235988	344720.857298	42.282816
3504.332267	344713.358890	42.287821
3504.120265	344711.559866	42.292826
3504.121316	344696.440502	42.297831
3504.081602	344695.810548	42.302836
3504.293188	344689.464763	42.307840
3504.385271	344695.890009	42.312845
3504.155049	344690.810380	42.317850
3504.472741	344671.822946	42.322855
3504.485404	344681.340608	42.327860
3504.341845	344680.472537	42.332864
3504.195511	344665.529186	42.337869
3504.104358	344651.442523	42.342874
3504.066357	344645.696167	42.347879
3504.102891	344643.628767	42.352884
3504.151732	344648.126397	42.357888
3504.328984	344655.352691	42.362893
3504.047998	344645.877648	42.367898
3503.971373	344634.359476	42.372903
3504.089734	344629.962881	42.377908
3504.215182	344628.695934	42.382912
3504.348185	344635.521972	42.387917
3504.409935	344624.872791	42.392922
3504.467608	344611.577099	42.397927
3504.551043	344600.848126	42.402932
3504.490240	344598.134325	42.407936
3504.435120	344583.660148	42.412941
3504.141416	344585.259340	42.417946
3504.345388	344580.365592	42.422951
3504.102025	344576.917049	42.427956
3504.307723	344580.753550	42.432960
3504.295977	344554.767564	42.437965
3503.936143	344547.519417	42.442970
3504.165249	344541.730823	42.447975
3504.202866	344560.713236	42.452980
3504.332879	344561.354572	42.457984
3504.107627	344538.660370	42.462989
3503.879821	344530.551386	42.467994
3504.281021	344522.444773	42.472999
3504.357060	344534.268703	42.478004
3504.198034	344529.101443	42.483008
3504.040201	344532.842699	42.488013
3503.822041	344515.161694	42.493018
3504.207849	344501.381393	42.498023
3504.159019	344508.261645	42.503028
3504.303540	344498.897483	42.508032
3504.274837	344499.233016	42.513037
3503.744078	344504.509531	42.518042
3504.271423	344499.411933	42.523047
3504.106940	344486.125880	42.528052
3503.889827	344481.985938	42.533056
3503.949967	344483.860088	42.538061
3504.154551	344476.777237	42.543066
3504.079062	344488.752398	42.548071
3504.381188	344494.609938	42.553076
3504.200332	344472.723202	42.558080
3504.276242	344465.202530	42.563085
3504.148684	344468.455388	42.568090
3504.445925	344457.132611	42.573095
3504.375364	344455.336671	42.578100
3504.512016	344442.766606	42.583104
3504.527778	344443.807808	42.588109
3504.438803	344435.244153	42.593114
3504.606549	344419.054773	42.598119
3504.436683	344412.031112	42.603124
3504.286407	344407.473342	42.608128
3504.368074	344376.101822	42.613133
3504.359069	344374.957939	42.618138
3504.562075	344372.787852	42.623143
3504.382780	344378.161535	42.628148
3504.239821	344363.777551	42.633152
3504.097980	344346.440779	42.638157
3504.279651	344352.011933	42.643162
3504.344080	344346.758424	42.648167
3504.054105	344348.382486	42.653172
3504.445828	344336.357505	42.658176
3504.324863	344325.838970	42.663181
3503.864829	344334.260556	42.668186
3504.203805	344323.363865	42.673191
3503.764917	344338.196396	42.678196
3503.907256	344328.985272	42.683200
3503.888384	344340.900606	42.688205
3504.085693	344334.124331	42.693210
3504.568701	344313.634342	42.698215
3503.958325	344324.192340	42.703220
3504.102507	344310.297473	42.708224
3504.421571	344308.770828	42.713229
3504.297339	344304.463468	42.718234
3504.477361	344281.017851	42.723239
3504.562453	344284.797078	42.728244
3504.350567	344277.780044	42.733248
3504.303191	344262.286423	42.738253
3504.090642	344257.534858	42.743258
3504.234588	344241.476459	42.748263
3504.032059	344263.144104	42.753268
3504.026079	344259.938003	42.758272
3504.447201	344243.708518	42.763277
3504.501721	344242.121879	42.768282
3504.560627	344233.891166	42.773287
3504.323394	344235.023275	42.778292
3504.294191	344211.534347	42.783296
3503.884275	344200.119688	42.788301
3504.143412	344203.667777	42.793306
3504.497585	344192.437763	42.798311
3504.186545	344203.915696	42.803316
3504.344607	344184.749714	42.808321
3504.211692	344179.731017	42.813325
3503.903240	344174.052824	42.818330
3504.128807	344180.558838	42.823335
3504.431504	344172.315029	42.828340
3504.183770	344165.405463	42.833345
3504.194422	344158.429595	42.838349
3504.016464	344152.323512	42.843354
3504.250367	344151.243037	42.848359
3504.149402	344152.022708	42.853364
3504.342350	344148.072451	42.858369
3504.280710	344130.239318	42.863373
3504.130199	344136.753885	42.868378
3504.522260	344118.543578	42.873383
3504.501715	344121.015928	42.878388
3504.356661	344109.177575	42.883393
3504.189969	344089.782914	42.888397
3504.119058	344093.561362	42.893402
3504.421084	344091.375611	42.898407
3504.165595	344071.002290	42.903412
3504.000374	344072.072110	42.908417
3504.521844	344056.335782	42.913421
3504.234755	344064.933694	42.918426
3504.352079	344053.282933	42.923431
3504.110621	344048.841365	42.928436
3504.182820	344030.554331	42.933441
3504.198530	344029.151998	42.938445
3503.808663	344039.675185	42.943450
3504.378345	344034.723576	42.948455
3504.183064	344030.911048	42.953460
3504.045752	344007.973658	42.958465
3504.312796	344008.364253	42.963469
3504.279900	344008.751360	42.968474
3504.087251	344007.254698	42.973479
3504.229995	344013.188389	42.978484
3504.052251	343983.435799	42.983489
3503.991082	343978.125752	42.988493
3503.811893	343985.230304	42.993498
3504.080392	343973.962886	42.998503
3503.971825	343987.521506	43.003508
3504.109969	343989.077896	43.008513
3504.137788	343991.389883	43.013517
3504.221990	343985.802318	43.018522
3504.201025	343962.439257	43.023527
3504.198063	343960.963513	43.028532
3504.088012	343961.642808	43.033537
3504.273383	343958.457347	43.038541
3503.821769	343969.881187	43.043546
3504.162113	343942.413863	43.048551
3504.234034	343934.002875	43.053556
3503.978175	343933.101639	43.058561
3504.205763	343927.720484	43.063565
3503.958952	343935.802972	43.068570
3504.509871	343937.217745	43.073575
3504.110254	343923.434211	43.078580
3504.068285	343924.331827	43.083585
3504.213159	343919.472822	43.088589
3503.764201	343929.394481	43.093594
3504.232009	343928.149756	43.098599
3504.205762	343929.808497	43.103604
3504.000743	343921.212206	43.108609
3504.387674	343898.166440	43.113613
3504.165829	343892.372713	43.118618
3504.542669	343878.313695	43.123623
3504.161059	343885.781157	43.128628
3504.317335	343856.713855	43.133633
3504.514013	343860.348200	43.138637
3504.159812	343865.367774	43.143642
3504.397400	343852.399821	43.148647
3504.123942	343842.236207	43.153652
3504.262666	343833.458292	43.158657
3504.558555	343827.964515	43.163661
3504.132930	343827.115569	43.168666
3504.322254	343819.831423	43.173671
3504.193313	343810.052217	43.178676
3504.579538	343798.791608	43.183681
3504.315656	343784.833861	43.188685
3504.154131	343796.059151	43.193690
3504.545137	343768.100116	43.198695
3504.442807	343771.578107	43.203700
3503.985174	343766.279812	43.208705
3504.283188	343769.541789	43.213709
3504.172048	343755.483526	43.218714
3504.563619	343732.971492	43.223719
3503.919953	343747.327468	43.228724
3504.400126	343735.542920	43.233729
3504.130062	343733.473052	43.238733
3503.798042	343725.685878	43.243738
3504.447821	343702.114860	43.248743
3504.310038	343714.558194	43.253748
3504.147896	343715.372996	43.258753
3504.407629	343706.041402	43.263757
3504.147156	343695.112096	43.268762
3504.356470	343682.123122	43.273767
3503.845976	343698.927075	43.278772
3504.095804	343679.390070	43.283777
3504.325495	343678.386614	43.288781
3504.134025	343680.147844	43.293786
3504.450853	343644.818874	43.298791
3504.230744	343654.042601	43.303796
3504.115483	343644.337566	43.308801
3504.315494	343649.854979	43.313805
3504.105686	343635.277757	43.318810
3503.887967	343627.014331	43.323815
3503.888004	343630.450693	43.328820
3503.865585	343621.265506	43.333825
3504.095762	343614.483953	43.338829
3503.920346	343630.369522	43.343834
3504.118405	343631.280103	43.348839
3504.261992	343632.784733	43.353844
3504.279829	343610.509914	43.358849
3504.280268	343600.099327	43.363853
3504.163798	343605.463147	43.368858
3504.403222	343591.603963	43.373863
3503.850252	343604.062050	43.378868
3504.117868	343582.154994	43.383873
3504.113894	343569.606976	43.388877
3504.049244	343572.722668	43.393882
3503.946159	343566.630142	43.398887
3503.885689	343564.043510	43.403892
3503.739360	343569.895677	43.408897
3503.852589	343577.055863	43.413901
3503.754165	343584.071332	43.418906
3504.090773	343573.607594	43.423911
3503.892252	343587.944142	43.428916
3503.818840	343579.123365	43.433921
3504.097429	343545.633059	43.438925
3504.094348	343552.531643	43.443930
3504.110284	343549.525670	43.448935
3504.165771	343558.451303	43.453940
3504.006593	343561.709208	43.458945
3503.777902	343554.312938	43.463949
3504.046041	343563.128590	43.468954
3504.179804	343546.740714	43.473959
3504.022315	343535.464198	43.478964
3504.068339	343524.690037	43.483969
3504.013212	343527.244240	43.488973
3504.165655	343533.609162	43.493978
3504.082144	343535.047883	43.498983
3504.063813	343532.276410	43.503988
3503.876507	343520.164628	43.508993
3503.747709	343498.192941	43.513997
3503.637119	343505.363066	43.519002
3503.913103	343499.770590	43.524007
3503.867034	343504.359673	43.529012
3503.535899	343499.015902	43.534017
3503.872484	343508.126188	43.539021
3503.480491	343510.530017	43.544026
3504.187147	343503.520400	43.549031
3504.135179	343514.524792	43.554036
3504.337575	343513.907457	43.559041
3504.447840	343505.388531	43.564045
3504.167207	343516.810881	43.569050
3504.108935	343500.809706	43.574055
3504.070772	343499.721323	43.579060
3503.998032	343500.598356	43.584065
3504.090565	343501.296537	43.589069
3504.166004	343505.204610	43.594074
3504.142475	343492.659667	43.599079
3503.964128	343479.579212	43.604084
3503.721848	343476.384972	43.609089
3504.396255	343471.594938	43.614093
3503.791963	343470.417879	43.619098
3504.038767	343468.699005	43.624103
3504.274218	343475.356257	43.629108
3504.104826	343483.375659	43.634113
3504.030087	343452.613818	43.639117
3504.004600	343452.490679	43.644122
3504.355902	343444.977249	43.649127
3504.059774	343443.318754	43.654132
3504.345214	343445.462765	43.659137
3504.351226	343448.669107	43.664141
3504.319776	343438.670796	43.669146
3504.419185	343415.084859	43.674151
3504.103676	343417.578416	43.679156
3503.864759	343430.088706	43.684161
3504.341431	343410.999374	43.689165
3504.114897	343407.268109	43.694170
3504.251120	343394.086996	43.699175
3504.051863	343384.955185	43.704180
3504.093920	343388.384917	43.709185
3504.622371	343387.283317	43.714189
3504.147869	343372.875146	43.719194
3504.020302	343359.124835	43.724199
3504.287588	343355.366405	43.729204
3504.372844	343348.811364	43.734209
3504.171369	343353.755928	43.739213
3503.996904	343337.314908	43.744218
3504.229614	343327.325724	43.749223
3503.850634	343337.745498	43.754228
3503.643301	343332.025784	43.759233
3504.307344	343329.070062	43.764237
3503.982768	343333.957727	43.769242
3504.020159	343333.111937	43.774247
3504.081756	343330.887806	43.779252
3504.412896	343314.214123	43.784257
3503.972361	343300.029651	43.789261
3503.900454	343305.946440	43.794266
3504.290469	343295.245125	43.799271
3504.304436	343309.089975	43.804276
3504.071298	343288.891030	43.809281
3504.256288	343279.978450	43.814285
3503.906536	343276.368472	43.819290
3504.059931	343266.162731	43.824295
3504.379207	343275.657599	43.829300
3504.184922	343269.706731	43.834305
3504.331621	343255.149416	43.839309
3504.023698	343242.369388	43.844314
3504.207812	343240.456787	43.849319
3504.098998	343243.044944	43.854324
3503.931686	343251.064048	43.859329
3504.654012	343237.332071	43.864333
3504.343324	343227.479686	43.869338
3504.468901	343213.409327	43.874343
3504.319992	343211.193017	43.879348
3504.277267	343200.000110	43.884353
3504.472104	343181.209802	43.889357
3504.127259	343175.206365	43.894362
3504.171047	343173.494125	43.899367
3504.075107	343182.418299	43.904372
3503.770518	343160.805183	43.909377
3504.095809	343139.754284	43.914381
3503.897675	343145.309233	43.919386
3504.003822	343151.223343	43.924391
3504.095660	343146.041757	43.929396
3503.969652	343146.316319	43.934401
3504.111896	343144.181248	43.939405
3504.172074	343156.084321	43.944410
3504.233113	343131.384362	43.949415
3503.594864	343123.670976	43.954420
3503.997090	343113.374963	43.959425
3504.113401	343112.083974	43.964429
3503.539934	343113.371076	43.969434
3503.850121	343117.725689	43.974439
3503.859300	343117.393436	43.979444
3503.832667	343119.637704	43.984449
3503.948095	343120.943167	43.989453
3503.658428	343129.668890	43.994458
3503.625362	343125.270670	43.999463
3503.665003	343129.209880	44.004468
3503.780118	343135.402567	44.009473
3504.175940	343124.725758	44.014477
3503.971761	343138.808767	44.019482
3504.218787	343125.406446	44.024487
3504.145134	343110.018495	44.029492
3503.990236	343104.901367	44.034497
3504.273599	343095.693213	44.039501
3503.963123	343102.538629	44.044506
3504.240784	343095.036797	44.049511
3503.913925	343097.710340	44.054516
3503.644284	343084.287875	44.059521
3504.058835	343072.335393	44.064525
3503.802168	343075.812370	44.069530
3503.902148	343075.313038	44.074535
3503.840357	343081.660968	44.079540
3503.845156	343076.620407	44.084545
3503.822196	343079.602263	44.089549
3503.943332	343083.604955	44.094554
3504.166425	343083.773419	44.099559
3503.718514	343088.960597	44.104564
3503.968823	343090.753818	44.109569
3504.344956	343080.283746	44.114573
3503.834432	343075.706465	44.119578
3504.024839	343068.040245	44.124583
3504.207784	343064.116952	44.129588
3504.204144	343059.255902	44.134593
3504.110128	343064.005323	44.139597
3503.930457	343073.731827	44.144602
3504.214730	343059.992700	44.149607
3503.939041	343047.538438	44.154612
3503.872684	343033.702012	44.159617
3504.285271	343027.247912	44.164621
3504.208238	343035.889125	44.169626
3504.320379	343033.351544	44.174631
3504.023914	343037.878431	44.179636
3503.813200	343024.675724	44.184641
3504.046844	343006.337400	44.189645
3503.856796	343012.247441	44.194650
3503.948408	342997.953314	44.199655
3504.318563	343006.625650	44.204660
3503.936522	343000.882616	44.209665
3504.244034	342996.685085	44.214669
3504.141581	343006.653933	44.219674
3504.109863	342997.062856	44.224679
3503.986821	342980.868149	44.229684
3504.068760	342972.404535	44.234689
3504.210783	342973.756705	44.239693
3503.919420	342979.377317	44.244698
3504.153629	342982.242158	44.249703
3503.996276	342970.761882	44.254708
3503.941286	342967.436189	44.259713
3504.082706	342953.312356	44.264717
3504.082646	342948.068919	44.269722
3503.996411	342946.071779	44.274727
3504.092394	342956.671071	44.279732
3504.056798	342952.324146	44.284737
3504.132979	342954.475803	44.289741
3503.750474	342940.612975	44.294746
3503.976956	342923.039381	44.299751
3504.038633	342918.804347	44.304756
3503.673518	342929.018366	44.309761
3504.158403	342916.392927	44.314765
3503.897729	342927.201334	44.319770
3504.014378	342922.244894	44.324775
3504.137937	342932.661651	44.329780
3503.841549	342927.617785	44.334785
3504.111283	342918.259034	44.339789
3503.576290	342930.587147	44.344794
3503.820558	342916.319776	44.349799
3504.261897	342894.665000	44.354804
3503.895475	342892.992148	44.359809
3504.264377	342899.781091	44.364813
3504.040463	342900.274766	44.369818
3504.235014	342892.633324	44.374823
3504.120103	342896.266079	44.379828
3504.162033	342885.390634	44.384833
3504.040242	342863.519425	44.389837
3504.131179	342866.636010	44.394842
3504.038519	342867.439838	44.399847
3503.986549	342870.884466	44.404852
3504.044660	342875.202585	44.409857
3504.209705	342867.514895	44.414861
3504.132660	342854.112839	44.419866
3504.155405	342840.160466	44.424871
3504.020828	342837.661881	44.429876
3504.109202	342843.400651	44.434881
3504.291423	342835.532064	44.439885
3503.857137	342841.506188	44.444890
3503.866680	342812.257944	44.449895
3503.622191	342797.915088	44.454900
3503.622596	342798.271484	44.459905
3503.576528	342805.380584	44.464909
3503.682840	342819.236401	44.469914
3504.113159	342816.801234	44.474919
3504.171738	342815.366641	44.479924
3503.804469	342816.239338	44.484929
3504.090584	342808.532501	44.489933
3504.004994	342825.727698	44.494938
3503.833796	342821.987647	44.499943
3503.950688	342815.402093	44.504948
3504.240376	342821.821756	44.509953
3504.181055	342811.191392	44.514957
3503.964478	342796.156861	44.519962
3503.973153	342783.352138	44.524967
3503.945685	342788.752868	44.529972
3503.889822	342789.270884	44.534977
3504.218031	342785.859146	44.539981
3504.082399	342795.044195	44.544986
3504.261941	342784.299701	44.549991
3504.036279	342771.684748	44.554996
3503.943115	342760.016104	44.560001
3504.261752	342759.762197	44.565005
3504.140359	342759.348768	44.570010
3504.077619	342755.158846	44.575015
3503.615030	342760.526552	44.580020
3503.857224	342766.419191	44.585025
3503.916084	342760.148255	44.590029
3503.713417	342766.900303	44.595034
3503.957589	342754.669244	44.600039
3504.056349	342738.999400	44.605044
3503.648638	342737.485797	44.610049
3503.642911	342738.937693	44.615053
3503.870307	342740.149100	44.620058
3503.933615	342738.484670	44.625063
3504.095475	342745.077274	44.630068
3503.866928	342738.724503	44.635073
3504.087982	342737.569672	44.640077
3504.248767	342735.075296	44.645082
3503.882300	342748.598606	44.650087
3504.150114	342718.825856	44.655092
3503.730996	342715.684986	44.660097
3503.913272	342712.143590	44.665101
3503.787813	342717.890723	44.670106
3504.005190	342705.918432	44.675111
3503.630825	342713.130352	44.680116
3503.592146	342722.910985	44.685121
3504.121250	342715.140267	44.690125
3503.613155	342718.860647	44.695130
3504.003943	342714.548114	44.700135
3504.095634	342722.195437	44.705140
3504.000858	342718.010577	44.710145
3504.131403	342705.237479	44.715149
3503.753356	342699.748327	44.720154
3503.962603	342694.420870	44.725159
3503.970922	342685.307044	44.730164
3503.731363	342683.665039	44.735169
3504.392008	342691.527869	44.740173
3503.935060	342691.498394	44.745178
3503.904193	342689.441583	44.750183
3504.025252	342689.778904	44.755188
3503.911257	342704.000482	44.760193
3503.833706	342694.518420	44.765197
3503.543081	342678.222855	44.770202
3504.175342	342676.773926	44.775207
3504.085606	342673.148259	44.780212
3503.809579	342677.595580	44.785217
3504.411002	342660.471719	44.790221
3504.054938	342668.317107	44.795226
3504.252996	342655.991501	44.800231
3504.237858	342661.619382	44.805236
3504.386321	342646.908917	44.810241
3504.459042	342643.588470	44.815245
3503.981301	342647.329509	44.820250
3504.257585	342646.955027	44.825255
3504.410997	342626.007485	44.830260
3504.169891	342613.471302	44.835265
3504.056006	342607.354932	44.840269
3504.270184	342606.532091	44.845274
3504.092752	342609.716571	44.850279
3503.786542	342613.252315	44.855284
3503.944767	342596.987585	44.860289
3504.221068	342575.155153	44.865293
3503.914505	342579.225494	44.870298
3504.103548	342576.777553	44.875303
3504.018374	342567.500310	44.880308
3503.539418	342579.386913	44.885313
3503.948177	342578.100588	44.890317
3503.868807	342582.720460	44.895322
3503.948454	342581.511618	44.900327
3503.696162	342585.293383	44.905332
3504.082363	342587.930580	44.910337
3504.183632	342572.871199	44.915341
3503.887704	342558.307330	44.920346
3504.024089	342545.507820	44.925351
3503.886291	342547.260598	44.930356
3503.938156	342560.412363	44.935361
3504.155239	342550.145524	44.940365
3504.059134	342553.648055	44.945370
3504.215223	342546.292647	44.950375
3503.832806	342529.146107	44.955380
3504.009351	342529.245569	44.960385
3504.387512	342516.331468	44.965389
3504.287392	342525.918212	44.970394
3503.822929	342535.384375	44.975399
3504.110827	342532.538989	44.980404
3503.959755	342517.214036	44.985409
3503.692357	342485.896710	44.990413
3503.990500	342494.631413	44.995418
3503.861804	342483.222876	45.000423
3503.812674	342495.601538	45.005428
3503.563406	342492.281078	45.010433
3503.954160	342488.019443	45.015437
3503.519510	342493.917296	45.020442
3503.826581	342496.057922	45.025447
3503.495639	342484.121364	45.030452
3503.833657	342497.991532	45.035457
3503.868053	342486.557212	45.040461
3503.641958	342508.636485	45.045466
3504.130606	342495.348551	45.050471
3503.972936	342515.864291	45.055476
3503.608842	342509.405653	45.060481
3504.104630	342506.731035	45.065485
3503.704056	342508.270813	45.070490
3503.923696	342514.930671	45.075495
3503.975132	342514.235375	45.080500
3503.911302	342506.023829	45.085505
3504.040113	342488.312824	45.090509
3503.815813	342486.872036	45.095514
3504.119248	342482.547842	45.100519
3504.164169	342480.377225	45.105524
3503.945974	342476.619129	45.110529
3504.045853	342478.792511	45.115533
3503.977229	342484.148867	45.120538
3504.021696	342480.145611	45.125543
3503.808601	342469.921313	45.130548
3504.176205	342455.354337	45.135553
3504.162326	342445.836715	45.140557
3503.996443	342451.692082	45.145562
3504.613914	342439.249217	45.150567
3503.931204	342433.350028	45.155572
3503.874087	342450.897191	45.160577
3504.396940	342423.603955	45.165581
3503.914822	342419.480310	45.170586
3503.979882	342417.051964	45.175591
3503.820530	342421.837218	45.180596
3503.625644	342421.842675	45.185601
3503.768558	342416.169320	45.190605
3503.516690	342426.874607	45.195610
3504.016979	342425.573807	45.200615
3503.970327	342422.221312	45.205620
3504.078047	342421.338936	45.210625
3504.042022	342427.097412	45.215629
3503.915395	342422.637569	45.220634
3504.004862	342402.769142	45.225639
3503.706168	342399.329219	45.230644
3503.986570	342387.041449	45.235649
3503.799963	342388.369224	45.240653
3503.844401	342397.016778	45.245658
3503.707909	342386.703992	45.250663
3503.779202	342398.783638	45.255668
3503.723237	342394.414439	45.260673
3503.983704	342400.355133	45.265677
3503.855670	342397.397317	45.270682
3503.979676	342400.203246	45.275687
3504.125462	342398.373041	45.280692
3503.958778	342407.333969	45.285697
3504.033022	342397.293321	45.290701
3503.556783	342389.936043	45.295706
3503.907167	342371.833615	45.300711
3503.976636	342372.179094	45.305716
3503.565061	342374.000613	45.310721
3504.016544	342366.598483	45.315725
3503.943669	342378.395472	45.320730
3503.851215	342365.021199	45.325735
3504.088586	342373.180076	45.330740
3503.930011	342378.677933	45.335745
3504.277595	342366.710445	45.340749
3504.055022	342379.040188	45.345754
3504.131195	342342.755782	45.350759
3504.250170	342346.249777	45.355764
3503.900087	342353.228811	45.360769
3504.007106	342342.062981	45.365773
3504.053439	342350.990240	45.370778
3504.126863	342339.040635	45.375783
3504.023150	342350.918868	45.380788
3503.574617	342323.015525	45.385793
3504.066705	342305.145219	45.390797
3503.701354	342321.392066	45.395802
3503.807238	342310.684588	45.400807
3503.857018	342321.953109	45.405812
3503.928046	342309.851151	45.410817
3504.377790	342314.540120	45.415821
3504.071749	342320.341294	45.420826
3503.959679	342324.711811	45.425831
3504.102350	342333.903840	45.430836
3504.076801	342311.813582	45.435841
3504.124896	342299.791610	45.440845
3503.833412	342287.950593	45.445850
3503.981309	342291.745472	45.450855
3504.346363	342280.411565	45.455860
3504.147117	342290.803103	45.460865
3504.342581	342286.190512	45.465869
3503.964256	342266.625084	45.470874
3504.013990	342253.381033	45.475879
3503.993512	342250.711659	45.480884
3504.172703	342261.297918	45.485889
3504.251854	342246.343770	45.490893
3503.986422	342262.473019	45.495898
3503.537866	342243.427774	45.500903
3504.090199	342254.667767	45.505908
3503.684449	342235.055756	45.510913
3503.754301	342224.735776	45.515917
3503.804987	342218.873347	45.520922
3503.996333	342217.977748	45.525927
3503.901496	342231.534592	45.530932
3504.018624	342227.112562	45.535937
3504.066980	342226.672294	45.540941
3503.970928	342237.658433	45.545946
3503.974591	342230.556173	45.550951
3503.987351	342229.841534	45.555956
3503.833638	342232.385923	45.560961
3504.034619	342228.866996	45.565965
3503.805758	342222.361493	45.570970
3503.778000	342202.358806	45.575975
3503.686893	342210.264183	45.580980
3503.466398	342209.993689	45.585985
3503.962311	342208.388125	45.590989
3503.858194	342205.121065	45.595994
3503.612729	342211.167217	45.600999
3503.709418	342212.501117	45.606004
3503.475224	342207.141904	45.611009
3503.914683	342211.654327	45.616013
3503.872206	342213.952041	45.621018
3503.950539	342215.365206	45.626023
3504.079156	342220.639493	45.631028
3503.595296	342218.527009	45.636033
3503.910741	342214.913622	45.641037
3503.647005	342225.951727	45.646042
3503.463082	342234.559043	45.651047
3503.929588	342225.194532	45.656052
3504.016106	342224.290050	45.661057
3503.980591	342222.972136	45.666061
3503.647432	342240.868452	45.671066
3503.664515	342235.494972	45.676071
3503.817451	342239.849054	45.681076
3503.896217	342243.756682	45.686081
3504.165453	342231.368829	45.691085
3504.108434	342217.250742	45.696090
3503.626893	342211.625181	45.701095
3503.695589	342199.905386	45.706100
3503.607026	342197.654045	45.711105
3503.793811	342207.450025	45.716109
3503.452493	342207.453178	45.721114
3504.047237	342193.512045	45.726119
3503.922601	342208.728144	45.731124
3503.767580	342207.581849	45.736129
3504.236878	342201.551422	45.741133
3503.937138	342211.042502	45.746138
3503.905134	342201.884069	45.751143
3504.271056	342211.295367	45.756148
3504.269410	342199.001241	45.761153
3504.189021	342172.388713	45.766157
3503.982780	342186.446814	45.771162
3503.941724	342163.900773	45.776167
3504.195518	342172.387989	45.781172
3504.011207	342176.540848	45.786177
3504.471744	342147.857346	45.791181
3503.938829	342150.105326	45.796186
3503.993704	342139.787699	45.801191
3503.934926	342132.746208	45.806196
3504.108303	342136.384342	45.811201
3504.109404	342129.384293	45.816205
3504.044667	342146.500022	45.821210
3504.130885	342129.661099	45.826215
3503.823989	342115.327948	45.831220
3503.851241	342117.869187	45.836225
3503.886514	342120.230977	45.841229
3503.652250	342115.609947	45.846234
3503.666340	342109.727839	45.851239
3504.002767	342103.947499	45.856244
3504.046448	342111.220672	45.861249
3504.229823	342102.231810	45.866253
3503.701341	342114.151787	45.871258
3504.106103	342113.247901	45.876263
3504.028808	342115.983850	45.881268
3503.854919	342106.236927	45.886273
3503.811027	342087.356750	45.891277
3504.072695	342076.980965	45.896282
3503.964502	342076.107264	45.901287
3503.971514	342065.822646	45.906292
3503.800451	342088.351551	45.911297
3503.962996	342086.340506	45.916301
3503.563088	342088.134734	45.921306
3503.857592	342085.364647	45.926311
3504.216906	342081.464317	45.931316
3504.229471	342087.978778	45.936321
3504.478290	342085.725003	45.941325
3504.243703	342060.791345	45.946330
3504.271610	342051.623419	45.951335
3503.952548	342050.681237	45.956340
3503.860924	342056.219447	45.961345
3504.066510	342050.765240	45.966349
3503.790710	342053.608937	45.971354
3503.651292	342035.125663	45.976359
3503.930766	342029.914318	45.981364
3503.715990	342014.675673	45.986369
3503.760135	342016.832428	45.991373
3503.666380	342022.447342	45.996378
3504.024118	342017.783622	46.001383
3503.883470	342017.551414	46.006388
3504.204162	342023.635351	46.011393
3504.158247	342011.602731	46.016397
3504.003597	342025.652712	46.021402
3503.959175	342030.267101	46.026407
3504.032739	342022.517404	46.031412
3503.570725	342008.106933	46.036417
3504.040690	341988.458216	46.041421
3503.862853	342000.450054	46.046426
3503.789366	341990.483603	46.051431
3503.924804	341996.138649	46.056436
3503.858079	342001.138384	46.061441
3504.188486	341989.351719	46.066445
3503.702640	342001.595887	46.071450
3504.106671	342003.059384	46.076455
3504.105170	341999.368818	46.081460
3503.615169	342002.780926	46.086465
3503.860945	342000.094903	46.091469
3503.986360	342008.958801	46.096474
3504.225170	341986.572086	46.101479
3503.834062	341964.946766	46.106484
3504.129172	341966.300211	46.111489
3504.370001	341959.134972	46.116493
3503.891563	341973.388881	46.121498
3503.667696	341969.402560	46.126503
3504.054939	341962.265082	46.131508
3503.734442	341977.995839	46.136513
3504.190545	341952.876579	46.141517
3503.855934	341950.282309	46.146522
3503.926127	341943.856771	46.151527
3503.913694	341932.149750	46.156532
3503.573244	341937.141855	46.161537
3503.771342	341934.208821	46.166541
3503.813776	341935.805849	46.171546
3503.707063	341945.928272	46.176551
3504.060872	341930.828807	46.181556
3503.852255	341939.032796	46.186561
3503.876816	341938.087196	46.191565
3503.866515	341947.099832	46.196570
3503.917608	341937.470041	46.201575
3504.261909	341941.819345	46.206580
3503.803527	341942.706459	46.211585
3504.137293	341910.071980	46.216589
3503.704982	341919.991336	46.221594
3503.221854	341912.991453	46.226599
3503.731087	341910.111047	46.231604
3503.407908	341921.082242	46.236609
3504.147749	341928.703560	46.241613
3504.200259	341923.858997	46.246618
3504.118201	341908.599343	46.251623
3504.276945	341910.457984	46.256628
3503.656591	341915.977978	46.261633
3504.031447	341901.766087	46.266637
3504.079857	341916.369447	46.271642
3504.219913	341907.463769	46.276647
3504.299900	341891.873038	46.281652
3504.319795	341875.935440	46.286657
3504.427875	341883.962095	46.291661
3503.813027	341881.768489	46.296666
3504.200570	341866.612766	46.301671
3503.920625	341864.391668	46.306676
3503.689128	341853.686539	46.311681
3504.087644	341853.420001	46.316685
3503.823036	341844.349197	46.321690
3503.913501	341845.658635	46.326695
3503.822605	341854.505843	46.331700
3503.773889	341848.608185	46.336705
3504.048026	341853.375861	46.341709
3503.623773	341854.868490	46.346714
3504.016504	341848.239223	46.351719
3504.121594	341852.600897	46.356724
3504.178959	341848.595561	46.361729
3504.129130	341831.778064	46.366733
3503.986067	341826.378956	46.371738
3503.834454	341823.221204	46.376743
3503.588235	341822.216593	46.381748
3503.779981	341813.150002	46.386753
3503.709331	341831.030391	46.391757
3503.772062	341828.347844	46.396762
3503.584761	341834.512110	46.401767
3503.752206	341820.663901	46.406772
3503.481767	341828.623132	46.411777
3503.684753	341818.282036	46.416781
3503.853925	341826.400859	46.421786
3503.572329	341824.790931	46.426791
3503.814063	341829.487368	46.431796
3503.861042	341822.938214	46.436801
3503.824322	341820.296844	46.441805
3503.954733	341839.239992	46.446810
3503.930047	341822.774881	46.451815
3503.856657	341839.764791	46.456820
3503.908361	341836.142168	46.461825
3504.257908	341829.392453	46.466829
3504.103835	341809.791426	46.471834
3503.499759	341804.516109	46.476839
3503.828582	341798.278759	46.481844
3503.723320	341799.899141	46.486849
3504.068484	341796.637395	46.491853
3503.713506	341801.580898	46.496858
3503.646864	341801.413353	46.501863
3504.025502	341799.749954	46.506868
3504.178141	341808.965941	46.511873
3503.964648	341811.952527	46.516877
3504.057607	341808.221562	46.521882
3503.725598	341807.357786	46.526887
3503.744865	341811.911213	46.531892
3503.719802	341810.515274	46.536897
3503.853910	341810.621447	46.541901
3504.054867	341800.204304	46.546906
3503.724959	341798.678377	46.551911
3504.077630	341784.673603	46.556916
3503.752463	341799.285141	46.561921
3504.177722	341793.796183	46.566925
3503.852146	341788.858654	46.571930
3503.986617	341797.237514	46.576935
3504.204743	341790.432208	46.581940
3503.846367	341787.918051	46.586945
3504.275923	341776.548399	46.591949
3503.871031	341766.354305	46.596954
3503.824251	341756.892686	46.601959
3504.292976	341759.924148	46.606964
3503.937080	341759.955059	46.611969
3503.785426	341773.877352	46.616973
3503.844439	341761.700821	46.621978
3503.801532	341760.867704	46.626983
3503.977504	341756.792702	46.631988
3503.560138	341769.280635	46.636993
3504.123586	341759.264361	46.641997
3503.868102	341765.363050	46.647002
3503.840071	341746.403896	46.652007
3504.004448	341730.901602	46.657012
3503.885838	341743.291400	46.662017
3503.888025	341730.232935	46.667021
3504.028840	341746.018093	46.672026
3504.267148	341731.955024	46.677031
3504.286618	341738.722976	46.682036
3503.783856	341736.257099	46.687041
3504.266386	341727.195433	46.692045
3503.816118	341710.746665	46.697050
3503.886986	341713.382844	46.702055
3503.952154	341707.008985	46.707060
3503.830358	341704.686515	46.712065
3503.804513	341703.214333	46.717069
3504.005823	341702.978972	46.722074
3504.065757	341705.795062	46.727079
3504.005579	341707.179227	46.732084
3503.686721	341710.971569	46.737089
3503.873206	341704.833076	46.742093
3503.755112	341714.550062	46.747098
3503.696205	341693.839404	46.752103
3503.786071	341692.272565	46.757108
3503.563347	341686.555128	46.762113
3503.806972	341689.647635	46.767117
3503.841356	341695.878687	46.772122
3504.038162	341686.709459	46.777127
3503.915866	341684.514340	46.782132
3503.828923	341689.262750	46.787137
3503.913326	341672.653080	46.792141
3503.830146	341679.895451	46.797146
3503.449584	341672.548414	46.802151
3504.105388	341671.350287	46.807156
3504.270675	341688.506142	46.812161
3504.155700	341689.084422	46.817165
3503.821614	341685.064598	46.822170
3503.836245	341685.927844	46.827175
3503.895688	341666.165742	46.832180
3503.699951	341642.880324	46.837185
3503.926017	341643.582871	46.842189
3504.030760	341650.362807	46.847194
3503.639853	341636.628282	46.852199
3503.843488	341653.039900	46.857204
3503.793471	341652.895181	46.862209
3504.110412	341641.339670	46.867213
3503.908116	341647.531780	46.872218
3503.873333	341648.886477	46.877223
3503.873622	341654.461103	46.882228
3503.919405	341652.875777	46.887233
3504.146577	341639.298086	46.892237
3503.937724	341632.102081	46.897242
3503.948874	341617.438531	46.902247
3504.104811	341610.312126	46.907252
3503.927551	341610.085705	46.912257
3503.879906	341616.431551	46.917261
3504.071055	341617.725076	46.922266
3503.754574	341616.655205	46.927271
3504.335204	341600.145248	46.932276
3503.896814	341616.123827	46.937281
3503.868943	341598.182789	46.942285
3503.716673	341590.977834	46.947290
3503.702716	341583.471011	46.952295
3504.040503	341578.148590	46.957300
3503.983224	341589.637809	46.962305
3503.816316	341592.006128	46.967309
3503.831659	341588.007419	46.972314
3503.612984	341589.391189	46.977319
3503.846348	341583.448910	46.982324
3503.580796	341589.676482	46.987329
3503.780009	341594.506932	46.992333
3503.790710	341593.130789	46.997338
3503.933648	341586.159165	47.002343
3503.982548	341591.827929	47.007348
3503.638667	341589.413292	47.012353
3503.860422	341592.865626	47.017357
3503.487364	341591.168333	47.022362
3503.717429	341601.568480	47.027367
3504.037810	341596.146994	47.032372
3503.733385	341602.024344	47.037377
3503.747897	341600.545780	47.042381
3504.171859	341602.693412	47.047386
3503.853261	341591.594733	47.052391
3503.743722	341582.677558	47.057396
3503.849314	341578.715489	47.062401
3504.099256	341569.716026	47.067405
3503.962499	341567.370462	47.072410
3503.909499	341570.484414	47.077415
3504.274228	341573.506871	47.082420
3504.036512	341577.897305	47.087425
3504.030411	341578.025644	47.092429
3504.114668	341550.292265	47.097434
3503.902344	341542.053156	47.102439
3503.974535	341538.274549	47.107444
3503.889139	341543.200908	47.112449
3504.223740	341520.646151	47.117453
3504.071881	341538.030370	47.122458
3503.928633	341527.871236	47.127463
3503.903793	341538.744423	47.132468
3503.905702	341540.602416	47.137473
3503.780616	341511.120286	47.142477
3503.892094	341515.888249	47.147482
3503.917733	341499.440550	47.152487
3503.786968	341491.799454	47.157492
3503.854431	341504.007155	47.162497
3503.938632	341498.419361	47.167501
3503.887465	341503.798497	47.172506
3503.936148	341501.601796	47.177511
3504.105697	341494.651409	47.182516
3503.979738	341513.762461	47.187521
3504.191111	341495.758116	47.192525
3503.916712	341487.656087	47.197530
3503.548478	341472.976116	47.202535
3503.911174	341468.362481	47.207540
3503.642211	341477.237895	47.212545
3503.640802	341472.147273	47.217549
3503.614071	341471.387958	47.222554
3503.813375	341469.778357	47.227559
3504.131340	341464.866337	47.232564
3503.677268	341471.200088	47.237569
3503.900061	341473.710440	47.242573
3503.909828	341483.203610	47.247578
3503.846219	341466.464556	47.252583
3503.805424	341471.256596	47.257588
3503.872747	341476.744275	47.262593
3504.301020	341473.622102	47.267597
3504.066927	341478.826522	47.272602
3504.267437	341465.303917	47.277607
3504.160635	341447.197130	47.282612
3504.020245	341437.750262	47.287617
3504.234182	341448.636625	47.292621
3504.052836	341444.516273	47.297626
3503.860768	341451.597702	47.302631
3504.133653	341446.285531	47.307636
3503.597807	341433.439336	47.312641
3503.858483	341400.612505	47.317645
3503.612212	341407.880691	47.322650
3503.323218	341410.548320	47.327655
3503.696194	341422.504100	47.332660
3503.767222	341450.111370	47.337665
3503.732908	341445.713226	47.342669
3503.915953	341446.677124	47.347674
3503.867886	341430.342878	47.352679
3503.886949	341416.925312	47.357684
3503.355545	341412.478479	47.362689
3503.703188	341411.761796	47.367693
3503.287333	341435.831471	47.372698
3503.818912	341441.322122	47.377703
3503.969929	341438.498327	47.382708
3503.498419	341436.587501	47.387713
3503.717790	341424.741918	47.392717
3503.765884	341447.389139	47.397722
3504.098257	341437.663892	47.402727
3504.042378	341424.970908	47.407732
3503.409810	341430.721969	47.412737
3503.909928	341416.439254	47.417741
3503.866382	341427.289963	47.422746
3503.908264	341421.530670	47.427751
3503.957673	341420.122948	47.432756
3504.109310	341437.790126	47.437761
3504.193738	341417.362172	47.442765
3504.061231	341435.048817	47.447770
3503.668103	341422.790972	47.452775
3504.005321	341399.421205	47.457780
3503.737340	341405.547360	47.462785
3503.870969	341394.402605	47.467789
3504.008201	341389.773698	47.472794
3504.024544	341396.236726	47.477799
3504.253386	341389.582410	47.482804
3504.104101	341399.915291	47.487809
3503.956779	341399.709590	47.492813
3503.883802	341393.382993	47.497818
3503.893008	341383.556099	47.502823
3503.958457	341364.149318	47.507828
3503.537943	341369.434129	47.512833
3503.758706	341361.151982	47.517837
3503.875723	341350.595305	47.522842
3503.510536	341362.184154	47.527847
3503.723846	341358.892321	47.532852
3503.878837	341364.544334	47.537857
3504.085168	341364.893638	47.542861
3504.033178	341371.520199	47.547866
3503.951757	341374.205923	47.552871
3503.960853	341363.284489	47.557876
3503.492255	341372.089660	47.562881
3503.925304	341366.141246	47.567885
3504.089675	341372.708148	47.572890
3503.882504	341378.722872	47.577895
3504.067135	341370.980989	47.582900
3503.888045	341365.332989	47.587905
3504.236309	341342.877826	47.592909
3504.162627	341342.660483	47.597914
3504.202973	341343.010573	47.602919
3504.146399	341337.674113	47.607924
3503.821644	341350.402038	47.612929
3503.945075	341346.513499	47.617933
3504.013357	341326.597162	47.622938
3503.688380	341313.819425	47.627943
3504.026878	341311.831447	47.632948
3503.809012	341317.033315	47.637953
3503.923927	341307.138788	47.642957
3504.099636	341312.914804	47.647962
3503.797657	341305.631665	47.652967
3504.026936	341314.071966	47.657972
3503.883522	341309.207419	47.662977
3503.722089	341311.473064	47.667981
3503.870115	341313.180689	47.672986
3504.007039	341315.322801	47.677991
3503.972714	341288.880792	47.682996
3503.901763	341283.266597	47.688001
3503.996649	341272.204310	47.693005
3503.858586	341286.964573	47.698010
3503.522586	341270.090345	47.703015
3503.866838	341271.359672	47.708020
3503.579154	341282.758100	47.713025
3503.619392	341289.573728	47.718029
3503.749747	341282.756787	47.723034
3503.909968	341282.375191	47.728039
3503.952148	341287.510495	47.733044
3503.576706	341283.751730	47.738049
3504.009807	341282.766988	47.743053
3503.980672	341283.128063	47.748058
3503.727313	341292.942864	47.753063
3504.186011	341289.103137	47.758068
3503.933066	341296.397846	47.763073
3503.909810	341280.288732	47.768077
3503.937031	341266.488021	47.773082
3503.931799	341247.652384	47.778087
3503.907033	341257.151048	47.783092
3503.820538	341251.768402	47.788097
3504.214934	341252.698890	47.793101
3503.969107	341252.992403	47.798106
3503.898773	341257.789130	47.803111
3504.173373	341244.203853	47.808116
3503.892979	341255.270221	47.813121
3504.174400	341255.302196	47.818125
3504.260703	341225.099230	47.823130
3504.092199	341229.886024	47.828135
3503.930505	341218.049736	47.833140
3503.841578	341218.242080	47.838145
3503.863641	341214.776835	47.843149
3503.999844	341223.053680	47.848154
3503.260234	341221.439780	47.853159
3504.040154	341214.341956	47.858164
3503.989286	341219.899253	47.863169
3503.810229	341211.680295	47.868173
3503.641498	341202.314236	47.873178
3503.612742	341203.362532	47.878183
3503.829009	341208.826688	47.883188
3503.684525	341196.758581	47.888193
3503.681599	341187.035394	47.893197
3503.567864	341199.602715	47.898202
3503.823314	341214.402602	47.903207
3503.995040	341210.455510	47.908212
3503.649256	341195.797379	47.913217
3504.036781	341183.186976	47.918221
3503.949496	341194.757377	47.923226
3503.962050	341192.464557	47.928231
3503.813919	341183.400696	47.933236
3503.649385	341197.299701	47.938241
3503.935855	341190.941711	47.943245
3503.934823	341192.214718	47.948250
3503.590578	341205.480305	47.953255
3503.822067	341198.596457	47.958260
3503.740273	341191.762137	47.963265
3503.883625	341190.466832	47.968269
3503.893573	341202.836415	47.973274
3503.819143	341210.688374	47.978279
3504.066784	341196.980075	47.983284
3503.618333	341193.538305	47.988289
3503.864986	341180.695623	47.993293
3503.553724	341172.981203	47.998298
3503.621677	341178.774268	48.003303
3504.289138	341178.821577	48.008308
3503.840989	341174.921571	48.013313
3503.906125	341176.158662	48.018317
3503.898767	341172.519883	48.023322
3503.736369	341174.989324	48.028327
3503.918417	341175.571561	48.033332
3503.630840	341180.504458	48.038337
3503.828188	341159.167646	48.043341
3504.019122	341178.432342	48.048346
3503.579026	341174.938340	48.053351
3504.196774	341170.258906	48.058356
3504.055271	341176.365088	48.063361
3503.886937	341161.984353	48.068365
3504.234849	341158.340317	48.073370
3504.097489	341135.478211	48.078375
3504.159982	341123.071910	48.083380
3503.914724	341143.932868	48.088385
3504.044858	341138.083232	48.093389
3503.640277	341134.354519	48.098394
3503.951843	341141.025449	48.103399
3504.193166	341131.849101	48.108404
3503.786406	341109.360489	48.113409
3503.758493	341105.979504	48.118413
3503.516224	341101.512392	48.123418
3503.559846	341096.898263	48.128423
3503.728680	341105.526333	48.133428
3503.461452	341111.143300	48.138433
3503.420238	341119.091839	48.143437
3503.878593	341140.350659	48.148442
3503.835844	341143.692106	48.153447
3503.912592	341145.614643	48.158452
3503.916038	341128.126705	48.163457
3504.134808	341114.041130	48.168461
3504.009646	341112.406451	48.173466
3504.065808	341108.961265	48.178471
3504.273810	341116.234032	48.183476
3503.998640	341127.579600	48.188481
3504.308190	341108.312332	48.193485
3503.881857	341091.528701	48.198490
3503.866461	341093.134894	48.203495
3503.760269	341075.995188	48.208500
3503.537287	341076.972372	48.213505
3503.802919	341078.865051	48.218509
3504.138968	341079.957495	48.223514
3503.829147	341083.926630	48.228519
3504.231823	341075.462956	48.233524
3503.939094	341081.898514	48.238529
3503.860779	341085.551046	48.243533
3504.221951	341074.421170	48.248538
3503.917556	341067.647482	48.253543
3503.906061	341046.954566	48.258548
3504.003968	341047.702836	48.263553
3503.950934	341048.347694	48.268557
3503.953447	341041.729123	48.273562
3503.624274	341047.915896	48.278567
3504.114018	341042.416677	48.283572
3503.783104	341058.174769	48.288577
3503.896892	341058.182336	48.293581
3503.819539	341049.030902	48.298586
3503.636715	341057.867303	48.303591
3503.948199	341043.232500	48.308596
3503.922720	341055.073160	48.313601
3504.092749	341040.460720	48.318605
3503.861695	341017.740658	48.323610
3503.702979	341022.195007	48.328615
3503.838504	341016.369961	48.333620
3503.748985	341018.089694	48.338625
3503.698954	341012.293984	48.343629
3503.950571	341014.621613	48.348634
3503.986082	341010.950592	48.353639
3504.090820	341018.366971	48.358644
3503.808809	341016.757087	48.363649
3503.702748	341013.286632	48.368653
3503.676561	341021.156442	48.373658
3503.466596	341024.473422	48.378663
3503.791644	341017.651127	48.383668
3503.770581	341028.472897	48.388673
3503.841700	341023.167133	48.393677
3503.717772	341031.637857	48.398682
3503.803216	341024.166161	48.403687
3503.923438	341011.903441	48.408692
3503.650864	341028.772334	48.413697
3504.072543	341020.509288	48.418701
3504.088069	341021.906955	48.423706
3503.882072	341002.822979	48.428711
3504.088916	340992.939323	48.433716
3503.857814	340991.092295	48.438721
3503.650498	340988.503314	48.443725
3503.626381	341000.801958	48.448730
3503.659537	340990.614847	48.453735
3503.958845	340985.603918	48.458740
3503.626485	340998.511302	48.463745
3503.735686	340992.232227	48.468749
3503.934306	340996.070076	48.473754
3503.709456	341003.029464	48.478759
3503.852553	340994.555908	48.483764
3503.668927	341006.497944	48.488769
3503.731322	340991.087951	48.493773
3503.865752	340992.594095	48.498778
3504.054470	340993.786198	48.503783
3503.973138	340995.708277	48.508788
3503.791107	341002.711805	48.513793
3503.923022	340996.683689	48.518797
3503.961129	340974.582887	48.523802
3503.960943	340968.270193	48.528807
3503.832553	340963.963253	48.533812
3503.888834	340965.379933	48.538817
3504.197696	340962.912985	48.543821
3503.850486	340968.695339	48.548826
3503.691266	340960.676852	48.553831
3504.063099	340961.127267	48.558836
3503.672570	340966.992835	48.563841
3503.906895	340961.483079	48.568845
3503.948355	340964.556673	48.573850
3503.613077	340959.824251	48.578855
3503.754121	340957.612929	48.583860
3504.010804	340966.761684	48.588865
3503.954678	340956.334132	48.593869
3504.315449	340940.138763	48.598874
3503.559901	340945.654760	48.603879
3503.782457	340932.764927	48.608884
3503.651478	340938.054910	48.613889
3503.660100	340931.002627	48.618893
3503.690566	340933.085218	48.623898
3503.780514	340937.067526	48.628903
3504.151569	340936.805326	48.633908
3503.793340	340940.374844	48.638913
3503.855478	340939.219649	48.643917
3503.766995	340948.193880	48.648922
3503.942418	340941.166138	48.653927
3504.009714	340940.391951	48.658932
3503.740446	340942.165559	48.663937
3503.891992	340953.036418	48.668941
3503.942650	340938.391916	48.673946
3503.530591	340914.478594	48.678951
3503.565112	340914.829608	48.683956
3503.606935	340939.412582	48.688961
3503.465580	340945.926043	48.693965
3503.687792	340948.054684	48.698970
3503.581882	340946.875146	48.703975
3503.971788	340944.522661	48.708980
3503.643012	340940.654677	48.713985
3503.667836	340948.134609	48.718989
3504.117340	340939.943518	48.723994
3503.583382	340936.846166	48.728999
3503.738292	340928.752557	48.734004
3503.402869	340939.369491	48.739009
3503.733009	340943.110187	48.744013
3503.549879	340958.081292	48.749018
3503.715972	340950.062283	48.754023
3503.981134	340952.667778	48.759028
3503.616483	340955.881941	48.764033
3503.748076	340966.730498	48.769037
3503.921189	340951.226626	48.774042
3503.861774	340945.152389	48.779047
3503.901782	340927.734979	48.784052
3503.618851	340924.368846	48.789057
3503.951963	340918.563464	48.794061
3503.983046	340917.820457	48.799066
3503.914867	340921.242301	48.804071
3504.240677	340915.158069	48.809076
3504.228212	340924.298471	48.814081
3503.677354	340927.898443	48.819085
3503.886129	340925.803687	48.824090
3503.648293	340917.772167	48.829095
3504.201830	340924.659416	48.834100
3504.193017	340906.206065	48.839105
3503.929141	340894.767694	48.844109
3503.876673	340900.859827	48.849114
3503.434693	340905.893520	48.854119
3504.074601	340894.108627	48.859124
3503.836630	340896.997306	48.864129
3503.721355	340903.073913	48.869133
3503.966769	340904.715244	48.874138
3503.709315	340893.632227	48.879143
3504.068824	340903.299289	48.884148
3503.830429	340907.460783	48.889153
3503.890374	340908.367786	48.894157
3504.028719	340901.422266	48.899162
3504.061719	340876.344005	48.904167
3504.112172	340865.161395	48.909172
3504.134493	340865.717976	48.914177
3503.849027	340863.039525	48.919181
3503.682549	340852.782133	48.924186
3503.926349	340867.583945	48.929191
3503.897651	340851.526489	48.934196
3503.615950	340858.902161	48.939201
3503.945417	340858.621081	48.944205
3504.066829	340863.463889	48.949210
3503.481812	340874.069384	48.954215
3503.648325	340865.413923	48.959220
3503.644408	340862.232770	48.964225
3503.476167	340872.925106	48.969229
3503.741980	340875.174131	48.974234
3503.567439	340873.979987	48.979239
3503.632953	340860.147678	48.984244
3503.704887	340883.860445	48.989249
3503.749461	340862.674959	48.994253
3503.982943	340872.311040	48.999258
3503.795607	340862.769686	49.004263
3504.060018	340870.924489	49.009268
3504.023599	340849.548163	49.014273
3503.813674	340851.541486	49.019277
3503.912611	340841.903961	49.024282
3503.655177	340838.355607	49.029287
3504.120889	340840.903946	49.034292
3503.799105	340836.525751	49.039297
3503.682048	340840.260787	49.044301
3503.751865	340840.708040	49.049306
3503.871743	340845.983827	49.054311
3504.140709	340836.523060	49.059316
3503.741824	340837.400783	49.064321
3503.843084	340836.850320	49.069325
3504.060148	340839.845249	49.074330
3504.023580	340828.778210	49.079335
3504.014155	340815.034103	49.084340
3503.628052	340807.891479	49.089345
3503.978266	340805.799813	49.094349
3504.199378	340810.855958	49.099354
3503.903332	340812.862898	49.104359
3503.705775	340811.876031	49.109364
3503.973615	340806.640968	49.114369
3503.834421	340816.183246	49.119373
3504.123401	340815.475831	49.124378
3504.100437	340805.857572	49.129383
3504.289920	340804.631332	49.134388
3504.256776	340778.290738	49.139393
3504.063905	340778.397696	49.144397
3504.504892	340772.397061	49.149402
3503.871265	340774.711921	49.154407
3504.121391	340767.952354	49.159412
3503.827897	340745.292974	49.164417
3504.089279	340742.909890	49.169421
3504.177151	340733.019547	49.174426
3503.986772	340731.242438	49.179431
3504.327808	340730.450428	49.184436
3504.302280	340731.650951	49.189441
3503.990688	340715.612730	49.194445
3504.107273	340699.404992	49.199450
3503.972789	340706.222851	49.204455
3503.820450	340702.276049	49.209460
3503.732616	340705.853743	49.214465
3504.014951	340700.718200	49.219469
3504.010048	340700.922716	49.224474
3503.649195	340698.383451	49.229479
3504.190499	340694.810634	49.234484
3503.715989	340704.380485	49.239489
3503.802104	340693.370391	49.244493
3503.931589	340684.720759	49.249498
3503.608998	340676.524422	49.254503
3503.779008	340667.613831	49.259508
3503.680765	340672.465925	49.264513
3503.639340	340661.195983	49.269517
3503.843247	340668.367630	49.274522
3503.454257	340673.163869	49.279527
3503.665008	340674.377950	49.284532
3503.755468	340676.323789	49.289537
3503.476557	340666.236871	49.294541
3503.959686	340680.211785	49.299546
3503.717580	340681.802920	49.304551
3503.682086	340664.066457	49.309556
3503.764941	340671.231786	49.314561
3503.916518	340674.491626	49.319565
3503.676037	340671.729690	49.324570
3503.724204	340677.245924	49.329575
3504.083036	340672.811026	49.334580
3503.772638	340670.721974	49.339585
3503.888059	340680.860396	49.344589
3503.854207	340671.982034	49.349594
3503.642195	340675.248445	49.354599
3503.691826	340683.589958	49.359604
3503.592621	340688.009467	49.364609
3503.837511	340696.116469	49.369613
3503.894315	340677.830862	49.374618
3503.706895	340692.369974	49.379623
3504.102590	340682.507323	49.384628
3503.627893	340695.513637	49.389633
3503.572148	340693.333417	49.394637
3504.030889	340690.053657	49.399642
3504.027878	340691.174257	49.404647
3503.923304	340686.710802	49.409652
3503.620682	340689.227885	49.414657
3503.926468	340691.419688	49.419661
3503.865174	340669.283582	49.424666
3503.610801	340657.945485	49.429671
3504.124554	340645.060467	49.434676
3503.420066	340655.786706	49.439681
3503.514496	340642.891614	49.444685
3504.044064	340645.124406	49.449690
3503.663529	340662.952303	49.454695
3504.024217	340654.444300	49.459700
3504.004396	340658.342160	49.464705
3504.126256	340655.573849	49.469709
3504.036720	340670.555682	49.474714
3503.741508	340661.845913	49.479719
3503.922420	340657.846423	49.484724
3504.025351	340653.502891	49.489729
3503.787978	340648.551326	49.494733
3504.033447	340638.763328	49.499738
3503.677953	340636.299579	49.504743
3503.842220	340622.222509	49.509748
3503.794095	340622.993870	49.514753
3503.801570	340629.025643	49.519757
3504.046708	340610.913883	49.524762
3503.652333	340622.609304	49.529767
3504.050198	340622.062859	49.534772
3504.022061	340612.089017	49.539777
3503.666410	340621.207353	49.544781
3503.740079	340615.188409	49.549786
3503.867036	340624.866824	49.554791
3504.053740	340623.437379	49.559796
3504.193048	340621.964517	49.564801
3504.216205	340619.364540	49.569805
3504.029202	340596.713725	49.574810
3503.615926	340602.379281	49.579815
3504.222600	340574.766517	49.584820
3504.028980	340587.982967	49.589825
3503.790636	340592.068109	49.594829
3503.833343	340579.384822	49.599834
3503.649014	340589.239730	49.604839
3503.940176	340577.662643	49.609844
3503.946640	340588.378317	49.614849
3503.656223	340581.856917	49.619853
3503.617185	340585.248717	49.624858
3503.685699	340599.645568	49.629863
3503.877529	340579.734916	49.634868
3503.856112	340586.051266	49.639873
3503.776704	340575.601877	49.644877
3503.685609	340560.801511	49.649882
3503.706189	340557.692836	49.654887
3503.718059	340547.610839	49.659892
3503.703437	340553.086099	49.664897
3503.982584	340554.671196	49.669901
3503.753009	340556.183988	49.674906
3503.428555	340555.853557	49.679911
3503.703836	340547.537228	49.684916
3503.808203	340552.993677	49.689921
3503.466069	340564.324479	49.694925
3503.584771	340573.902387	49.699930
3503.798830	340575.777779	49.704935
3503.945992	340571.859985	49.709940
3503.942735	340567.049587	49.714945
3503.783924	340576.060445	49.719949
3503.860246	340563.499116	49.724954
3503.597610	340561.529785	49.729959
3503.632470	340560.735267	49.734964
3503.619605	340551.573564	49.739969
3503.646726	340566.918806	49.744973
3503.705476	340562.073150	49.749978
3503.485404	340552.969660	49.754983
3503.689909	340565.537707	49.759988
3503.752554	340568.658882	49.764993
3503.782333	340566.108765	49.769997
3503.869754	340566.985974	49.775002
3503.851226	340563.883482	49.780007
3503.971668	340558.849887	49.785012
3503.692443	340577.603631	49.790017
3504.127052	340569.287571	49.795021
3504.023439	340573.453234	49.800026
3503.975210	340580.053830	49.805031
3503.817779	340568.064014	49.810036
3503.828404	340581.299086	49.815041
3503.670786	340575.265793	49.820045
3503.982311	340570.023804	49.825050
3503.428611	340565.325882	49.830055
3503.758215	340564.204761	49.835060
3503.605326	340576.218385	49.840065
3504.138951	340571.043104	49.845069
3504.248819	340561.861999	49.850074
3503.848550	340542.146762	49.855079
3503.940980	340540.477668	49.860084
3503.816721	340548.821235	49.865089
3503.732273	340546.009170	49.870093
3503.726174	340537.940965	49.875098
3503.965586	340554.347217	49.880103
3504.000448	340542.836098	49.885108
3503.967575	340550.121557	49.890113
3504.022735	340552.607539	49.895117
3504.098824	340545.442725	49.900122
3503.807710	340525.481130	49.905127
3504.200436	340511.291552	49.910132
3504.030588	340502.358301	49.915137
3503.734475	340501.947023	49.920141
3504.242263	340508.816096	49.925146
3503.800736	340510.642403	49.930151
3503.637166	340514.257536	49.935156
3503.822509	340514.890169	49.940161
3504.013193	340513.103721	49.945165
3504.254294	340499.218117	49.950170
3503.829647	340495.008891	49.955175
3503.906646	340480.792854	49.960180
3503.595546	340476.616586	49.965185
3503.771638	340474.246975	49.970189
3503.721399	340475.069583	49.975194
3503.381577	340486.680040	49.980199
3503.610797	340485.752973	49.985204
3503.275064	340484.864312	49.990209
3503.271500	340494.385196	49.995213
3503.333994	340516.012275	50.000218
3503.452237	340519.353758	50.005223
3503.931825	340514.110650	50.010228
3503.530823	340526.392605	50.015233
3503.199800	340533.496106	50.020237
3503.568798	340521.219415	50.025242
3503.641234	340525.891806	50.030247
3503.467809	340514.184514	50.035252
3503.534902	340524.432422	50.040257
3503.625484	340528.083740	50.045261
3503.785462	340521.134757	50.050266
3503.881147	340525.879838	50.055271
3503.897061	340521.015496	50.060276
3503.833804	340525.174782	50.065281
3503.754027	340528.522116	50.070285
3504.100996	340526.303678	50.075290
3503.909212	340536.108864	50.080295
3504.252671	340528.494497	50.085300
3504.002093	340532.836128	50.090305
3503.937543	340528.239058	50.095309
3503.597505	340510.550698	50.100314
3503.426258	340517.603486	50.105319
3503.744915	340516.051358	50.110324
3503.653426	340537.142760	50.115329
3503.806301	340537.805981	50.120333
3503.994144	340537.801840	50.125338
3504.018358	340517.841301	50.130343
3503.971860	340508.583089	50.135348
3503.704530	340506.792684	50.140353
3503.904924	340501.008246	50.145357
3504.127413	340503.976878	50.150362
3503.617366	340504.363076	50.155367
3504.140739	340493.920198	50.160372
3504.118088	340505.887790	50.165377
3503.370082	340508.806210	50.170381
3503.718025	340505.111221	50.175386
3503.612078	340504.618969	50.180391
3503.695933	340498.292942	50.185396
3503.752757	340503.298719	50.190401
3503.781273	340492.577703	50.195405
3504.078814	340495.916297	50.200410
3503.836701	340501.300252	50.205415
3503.892489	340499.051482	50.210420
3504.083269	340484.511997	50.215425
3504.143960	340475.465930	50.220429
3504.047613	340467.361074	50.225434
3503.950678	340473.383913	50.230439
3504.081471	340455.188364	50.235444
3503.860133	340470.063806	50.240449
3503.812109	340470.682423	50.245453
3504.197037	340463.265134	50.250458
3503.530007	340461.359732	50.255463
3503.985218	340460.906040	50.260468
3503.680879	340453.419532	50.265473
3503.818309	340451.641501	50.270477
3503.664535	340440.414737	50.275482
3503.784562	340453.657996	50.280487
3503.560229	340455.424513	50.285492
3503.763869	340444.090333	50.290497
3503.738721	340437.781532	50.295501
3503.935132	340448.747208	50.300506
3503.704032	340462.656899	50.305511
3503.908593	340453.078981	50.310516
3503.623627	340442.712977	50.315521
3503.743960	340452.341556	50.320525
3503.804484	340461.826859	50.325530
3503.392936	340452.269978	50.330535
3504.127493	340449.608435	50.335540
3504.243387	340453.357576	50.340545
3503.787401	340460.073559	50.345549
3504.069056	340459.749126	50.350554
3503.807123	340462.387062	50.355559
3503.870045	340453.111542	50.360564
3504.112285	340453.887912	50.365569
3503.967500	340431.561279	50.370573
3503.994183	340418.575031	50.375578
3503.930332	340416.701545	50.380583
3504.092970	340407.613895	50.385588
3504.085280	340419.604594	50.390593
3504.011696	340417.350819	50.395597
3504.251146	340404.076380	50.400602
3503.960676	340400.787775	50.405607
3503.979563	340388.897325	50.410612
3503.927659	340384.680074	50.415617
3503.779639	340376.710650	50.420621
3503.897022	340387.026995	50.425626
3503.421030	340391.913376	50.430631
3503.841054	340379.221307	50.435636
3503.766343	340389.389835	50.440641
3503.680547	340389.250769	50.445645
3503.991572	340373.419489	50.450650
3503.822447	340379.148288	50.455655
3503.625675	340375.081214	50.460660
3503.960304	340384.625014	50.465665
3503.629199	340388.699379	50.470669
3503.940186	340384.272025	50.475674
3503.855373	340383.903707	50.480679
3504.075424	340372.286913	50.485684
3503.694437	340380.085620	50.490689
3503.506176	340390.857568	50.495693
3503.819827	340375.458612	50.500698
3503.713633	340390.468601	50.505703
3503.629625	340383.838183	50.510708
3503.656809	340389.001386	50.515713
3503.725215	340378.350410	50.520717
3503.879676	340386.064465	50.525722
3503.777240	340380.251526	50.530727
3504.061257	340353.656970	50.535732
3504.075219	340339.145405	50.540737
3503.786711	340304.521135	50.545741
3503.749520	340260.362315	50.550746
3503.234495	340205.893266	50.555751
3503.452348	340154.744768	50.560756
3503.144286	340096.806444	50.565761
3503.063744	340013.071312	50.570765
3502.738881	339940.880517	50.575770
3502.060987	339852.708558	50.580775
3501.999133	339763.980885	50.585780
3501.572902	339672.052395	50.590785
3501.206540	339568.201131	50.595789
3501.249163	339452.906409	50.600794
3501.019368	339337.527267	50.605799
3500.057841	339222.161778	50.610804
3499.325945	339097.341171	50.615809
3498.741347	338982.552051	50.620813
3498.966511	338853.506742	50.625818
3498.075308	338733.089007	50.630823
3498.010311	338594.924951	50.635828
3497.363176	338455.147085	50.640833
3496.751298	338316.788878	50.645837
3496.568894	338164.285276	50.650842
3495.682353	338028.006361	50.655847
3495.343851	337882.603577	50.660852
3494.749077	337735.993629	50.665857
3494.109594	337578.978798	50.670861
3493.814583	337422.520084	50.675866
3492.933604	337273.434170	50.680871
3492.408822	337112.810738	50.685876
3491.835397	336955.936715	50.690881
3491.353412	336783.417515	50.695885
3490.660646	336624.601417	50.700890
3489.962211	336463.036511	50.705895
3489.421352	336302.846423	50.710900
3488.838335	336131.537977	50.715905
3488.492123	335965.079381	50.720909
3488.073605	335792.216647	50.725914
3486.905352	335633.524288	50.730919
3486.812033	335454.474130	50.735924
3486.269996	335280.967734	50.740929
3485.202860	335109.631407	50.745933
3484.798363	334924.366572	50.750938
3483.734686	334752.850602	50.755943
3483.541838	334573.992072	50.760948
3482.592436	334402.024382	50.765953
3482.021912	334221.926318	50.770957
3481.346933	334052.001891	50.775962
3480.470094	333869.685612	50.780967
3480.256554	333696.352404	50.785972
3479.611648	333509.237914	50.790977
3478.535307	333340.597187	50.795981
3478.555538	333162.821486	50.800986
3477.725155	332983.881464	50.805991
3476.936517	332795.896773	50.810996
3476.308048	332614.785417	50.816001
3475.550542	332443.291746	50.821005
3475.156383	332248.725940	50.826010
3474.155560	332074.113027	50.831015
3473.520838	331879.813381	50.836020
3473.180699	331697.304824	50.841025
3472.373021	331523.092833	50.846029
3471.942413	331337.771778	50.851034
3470.610651	331168.071592	50.856039
3470.571248	330972.275166	50.861044
3469.717399	330783.608154	50.866049
3468.872838	330605.453694	50.871053
3468.630352	330421.831781	50.876058
3467.734250	330237.345314	50.881063
3466.932709	330044.441955	50.886068
3466.323691	329872.384121	50.891073
3465.764365	329691.203655	50.896077
3465.235517	329500.394347	50.901082
3464.380998	329316.586432	50.906087
3463.910987	329130.527772	50.911092
3463.064699	328951.274892	50.916097
3462.179498	328767.979686	50.921101
3461.628682	328578.979154	50.926106
3460.624418	328397.153078	50.931111
3460.085369	328206.087540	50.936116
3459.591580	328031.512269	50.941121
3459.077583	327854.164684	50.946125
3458.463476	327661.531163	50.951130
3457.788874	327480.541904	50.956135
3456.788939	327298.508887	50.961140
3456.338596	327117.356030	50.966145
3454.947089	326938.261074	50.971149
3454.705861	326749.639968	50.976154
3454.174330	326578.733686	50.981159
3453.382560	326402.674295	50.986164
3452.746416	326217.016837	50.991169
3451.834203	326048.308277	50.996173
3451.180185	325860.132244	51.001178
3450.726075	325689.135442	51.006183
3450.244989	325492.860243	51.011188
3449.335376	325324.022457	51.016193
3448.485308	325144.990653	51.021197
3448.342841	324961.747401	51.026202
3447.351245	324781.693293	51.031207
3446.804112	324596.680039	51.036212
3446.128940	324434.932384	51.041217
3445.115078	324259.030779	51.046221
3444.839852	324060.224444	51.051226
3443.901820	323894.188937	51.056231
3443.316993	323709.612512	51.061236
3442.644820	323530.752789	51.066241
3442.046578	323355.802020	51.071245
3441.131423	323172.778865	51.076250
3440.330177	322997.986766	51.081255
3439.962819	322818.466276	51.086260
3439.419747	322648.775833	51.091265
3438.476031	322466.850528	51.096269
3438.066786	322294.108315	51.101274
3436.729688	322117.311316	51.106279
3436.652535	321934.051179	51.111284
3435.815871	321760.051488	51.116289
3435.007619	321591.521227	51.121293
3434.584954	321410.784417	51.126298
3433.779346	321233.850676	51.131303
3433.161206	321052.583885	51.136308
3432.934773	320887.626794	51.141313
3432.206191	320712.436710	51.146317
3431.472522	320525.432718	51.151322
3430.542072	320354.373241	51.156327
3429.763717	320165.796923	51.161332
3429.323820	319996.085080	51.166337
3428.440932	319821.019520	51.171341
3427.850946	319633.048872	51.176346
3427.346459	319456.013112	51.181351
3426.453995	319280.362405	51.186356
3425.898740	319110.336160	51.191361
3425.061103	318925.331411	51.196365
3424.843070	318739.489908	51.201370
3424.026234	318575.895142	51.206375
3423.458452	318391.483234	51.211380
3422.916082	318207.627127	51.216385
3421.787203	318037.485948	51.221389
3421.354060	317846.253154	51.226394
3420.787672	317686.207502	51.231399
3419.932244	317496.721331	51.236404
3419.049995	317319.537603	51.241409
3418.220143	317158.717926	51.246413
3418.292347	316966.512280	51.251418
3416.989177	316798.484446	51.256423
3416.535682	316624.261757	51.261428
3415.945968	316445.426016	51.266433
3415.028268	316281.690539	51.271437
3414.430754	316094.528950	51.276442
3413.659422	315926.975730	51.281447
3413.121717	315751.873618	51.286452
3412.803210	315572.815188	51.291457
3411.765000	315392.673470	51.296461
3411.485521	315221.883846	51.301466
3410.433211	315048.007750	51.306471
3409.859758	314869.777768	51.311476
3409.010191	314698.619080	51.316481
3407.803359	314523.340576	51.321485
3407.527984	314347.608918	51.326490
3406.975291	314192.113511	51.331495
3406.343644	314010.759228	51.336500
3405.526357	313852.453224	51.341505
3405.232403	313668.982390	51.346509
3404.630173	313498.495619	51.351514
3403.836012	313330.992736	51.356519
3402.922802	313150.521820	51.361524
3402.569784	312972.788515	51.366529
3401.878135	312796.101565	51.371533
3401.548878	312623.940548	51.376538
3400.351647	312451.865590	51.381543
3399.665007	312278.945696	51.386548
3399.163422	312102.125714	51.391553
3398.617052	311935.854713	51.396557
3397.939609	311766.650339	51.401562
3397.115248	311585.144230	51.406567
3396.753690	311412.197048	51.411572
3396.019915	311230.115828	51.416577
3395.345055	311067.097835	51.421581
3394.619023	310877.706545	51.426586
3393.700189	310717.833298	51.431591
3393.278062	310529.615671	51.436596
3392.496512	310360.756709	51.441601
3391.425275	310181.808407	51.446605
3391.285844	309999.809507	51.451610
3390.465384	309826.321365	51.456615
3389.508897	309663.091291	51.461620
3389.039840	309501.922949	51.466625
3388.229274	309316.616858	51.471629
3387.607346	309152.187263	51.476634
3386.741538	308985.733359	51.481639
3386.415388	308814.610204	51.486644
3385.481994	308658.632607	51.491649
3385.101446	308483.035765	51.496653
3384.611693	308300.987835	51.501658
3383.620763	308132.082453	51.506663
3382.831722	307960.190968	51.511668
3382.571905	307791.857061	51.516673
3381.826490	307618.735883	51.521677
3381.564344	307439.451867	51.526682
3380.331071	307272.544473	51.531687
3379.945397	307102.854433	51.536692
3379.330380	306920.467804	51.541697
3378.602107	306757.299667	51.546701
3378.123588	306566.461937	51.551706
3377.153497	306404.477541	51.556711
3376.537968	306228.558227	51.561716
3375.782794	306058.950726	51.566721
3374.954994	305888.565065	51.571725
3374.422353	305703.566239	51.576730
3373.687204	305550.864020	51.581735
3372.974625	305365.231082	51.586740
3372.160115	305199.298920	51.591745
3371.240014	305044.129752	51.596749
3371.147024	304864.866416	51.601754
3370.493013	304700.079689	51.606759
3369.688021	304528.568227	51.611764
3369.221851	304355.602354	51.616769
3368.566953	304183.990335	51.621773
3367.845515	304014.349500	51.626778
3367.115350	303849.752080	51.631783
3366.349337	303663.921598	51.636788
3365.576005	303499.890853	51.641793
3364.708776	303339.618264	51.646797
3364.298692	303161.039569	51.651802
3363.536695	303010.707170	51.656807
3362.824267	302831.870300	51.661812
3362.061915	302674.534458	51.666817
3361.312428	302509.047270	51.671821
3361.291653	302338.758888	51.676826
3360.194229	302182.290438	51.681831
3359.555634	302000.537760	51.686836
3359.031370	301842.628607	51.691841
3358.158661	301672.474217	51.696845
3357.551854	301498.610446	51.701850
3356.922411	301338.272654	51.706855
3356.206390	301165.571768	51.711860
3355.505930	301000.151602	51.716865
3355.277748	300845.072309	51.721869
3354.555712	300671.429582	51.726874
3353.579587	300502.512672	51.731879
3353.218777	300338.744355	51.736884
3352.366712	300172.634255	51.741889
3351.284138	300003.860996	51.746893
3351.242625	299836.680104	51.751898
3350.013452	299668.439019	51.756903
3349.514218	299510.447211	51.761908
3349.082095	299331.358308	51.766913
3348.281590	299174.050499	51.771917
3348.092723	298994.056904	51.776922
3347.037290	298840.252570	51.781927
3346.478954	298656.624392	51.786932
3346.144448	298502.145472	51.791937
3345.323235	298331.546551	51.796941
3344.793590	298142.234217	51.801946
3343.762439	297981.269132	51.806951
3343.127149	297806.616553	51.811956
3342.460082	297629.753216	51.816961
3341.716002	297477.044469	51.821965
3341.178949	297298.352103	51.826970
3340.654832	297144.131211	51.831975
3339.716806	296959.211614	51.836980
3339.380652	296801.599079	51.841985
3338.010992	296626.705000	51.846989
3337.645490	296462.577281	51.851994
3337.059792	296286.489286	51.856999
3336.172705	296116.968361	51.862004
3335.747767	295962.960035	51.867009
3334.788104	295791.998687	51.872013
3334.505794	295623.960645	51.877018
3333.765233	295456.555218	51.882023
3332.991776	295299.341712	51.887028
3332.379875	295134.666122	51.892033
3331.670405	294958.571066	51.897037
3330.981036	294795.460956	51.902042
3330.169805	294625.009966	51.907047
3329.839404	294466.910802	51.912052
3329.028187	294313.446210	51.917057
3328.397043	294147.117517	51.922061
3327.797218	293966.700324	51.927066
3326.983186	293791.715936	51.932071
3326.018787	293639.370192	51.937076
3325.794300	293463.069865	51.942081
3324.893958	293308.727310	51.947085
3324.335235	293137.191059	51.952090
3323.862175	292966.787163	51.957095
3322.972855	292814.021511	51.962100
3322.330559	292650.163813	51.967105
3321.597430	292488.612441	51.972109
3320.929691	292319.257565	51.977114
3320.123916	292157.641056	51.982119
3319.509174	291998.006158	51.987124
3319.153405	291830.562595	51.992129
3318.351793	291669.581794	51.997133
3317.815579	291494.831890	52.002138
3317.055905	291340.185669	52.007143
3315.983277	291176.344114	52.012148
3315.591808	291002.589682	52.017153
3314.842899	290852.423766	52.022157
3314.450409	290675.816902	52.027162
3313.589350	290524.395156	52.032167
3312.784017	290359.670380	52.037172
3312.424478	290197.345359	52.042177
3311.555179	290034.515114	52.047181
3310.967017	289879.993719	52.052186
3310.241651	289712.454458	52.057191
3309.729561	289550.305995	52.062196
3308.958317	289388.096560	52.067201
3308.136425	289230.886732	52.072205
3307.330179	289064.455001	52.077210
3306.500824	288904.724867	52.082215
3306.077133	288742.714781	52.087220
3305.442030	288587.614366	52.092225
3304.815334	288422.299934	52.097229
3304.338888	288269.746516	52.102234
3303.662553	288110.424719	52.107239
3303.142666	287950.696077	52.112244
3302.310029	287776.474652	52.117249
3301.817953	287622.446261	52.122253
3301.026221	287458.634575	52.127258
3300.100839	287294.691143	52.132263
3299.305932	287132.560686	52.137268
3299.027024	286970.857893	52.142273
3298.336405	286814.975911	52.147277
3297.711060	286656.485801	52.152282
3296.691907	286488.660221	52.157287
3296.351743	286327.272441	52.162292
3295.692158	286174.110351	52.167297
3295.157324	286016.318752	52.172301
3294.511324	285843.212910	52.177306
3293.987085	285682.592545	52.182311
3293.107338	285513.776695	52.187316
3292.581685	285352.163165	52.192321
3291.756046	285187.591789	52.197325
3291.376182	285031.634454	52.202330
3290.360842	284870.072726	52.207335
3289.488978	284699.421593	52.212340
3288.922193	284537.228489	52.217345
3288.482955	284386.297532	52.222349
3287.991051	284218.260264	52.227354
3286.650586	284061.053786	52.232359
3286.209264	283895.045851	52.237364
3285.484128	283729.286498	52.242369
3284.954347	283588.454999	52.247373
3284.336633	283415.369180	52.252378
3283.507775	283255.763908	52.257383
3283.200569	283098.622889	52.262388
3282.533151	282943.601727	52.267393
3281.508844	282786.930604	52.272397
3281.309372	282613.803828	52.277402
3280.202033	282462.774225	52.282407
3279.464783	282295.921201	52.287412
3279.167869	282141.452445	52.292417
3278.099321	281975.721402	52.297421
3277.474084	281822.272295	52.302426
3276.850574	281658.661038	52.307431
3276.354730	281497.932928	52.312436
3275.629348	281337.674049	52.317441
3275.020360	281183.534577	52.322445
3274.320691	281029.001922	52.327450
3273.360238	280871.326949	52.332455
3272.806309	280713.689509	52.337460
3272.607977	280563.407061	52.342465
3271.956998	280398.042542	52.347469
3271.270705	280243.405737	52.352474
3270.680925	280079.075674	52.357479
3270.068623	279923.077283	52.362484
3269.592364	279751.598069	52.367489
3268.477311	279596.061177	52.372493
3267.824413	279411.620992	52.377498
3267.092511	279259.436193	52.382503
3266.407871	279101.080555	52.387508
3265.629276	278949.819958	52.392513
3265.033668	278786.814951	52.397517
3264.559004	278622.390029	52.402522
3263.805708	278464.274379	52.407527
3262.978657	278309.073770	52.412532
3262.611109	278132.101405	52.417537
3261.730750	277989.108542	52.422541
3261.082054	277809.684713	52.427546
3260.336709	277667.867476	52.432551
3259.557888	277501.911501	52.437556
3259.088437	277347.240000	52.442561
3258.435436	277172.477502	52.447565
3257.977354	277023.865652	52.452570
3256.804510	276863.575003	52.457575
3256.355952	276698.025151	52.462580
3256.003642	276540.151517	52.467585
3254.720479	276392.281399	52.472589
3254.080961	276225.437376	52.477594
3253.658117	276073.789167	52.482599
3253.295162	275929.542781	52.487604
3252.409716	275768.569910	52.492609
3251.696991	275604.462568	52.497613
3251.280525	275445.682187	52.502618
3250.277265	275287.096508	52.507623
3249.974550	275127.712358	52.512628
3249.067688	274972.804347	52.517633
3248.520461	274810.861105	52.522637
3247.752046	274651.907192	52.527642
3247.200415	274497.274082	52.532647
3246.239882	274329.360228	52.537652
3245.928872	274178.789473	52.542657
3244.970649	274028.779544	52.547661
3244.342143	273866.721851	52.552666
3243.572136	273717.140593	52.557671
3243.076358	273559.060457	52.562676
3242.977280	273389.966168	52.567681
3241.802049	273232.884938	52.572685
3241.014329	273069.910158	52.577690
3240.435443	272923.915229	52.582695
3239.668708	272750.546060	52.587700
3239.372924	272600.838926	52.592705
3238.321059	272450.003471	52.597709
3238.005845	272281.936750	52.602714
3237.204731	272139.924650	52.607719
3236.435666	271965.715489	52.612724
3235.787767	271823.679185	52.617729
3235.218882	271655.652678	52.622733
3234.644638	271497.636106	52.627738
3233.976192	271355.297492	52.632743
3232.852031	271190.160423	52.637748
3232.263020	271015.540902	52.642753
3231.576250	270871.422472	52.647757
3231.146101	270718.400488	52.652762
3230.468728	270556.911222	52.657767
3229.779764	270412.360252	52.662772
3229.272403	270240.478543	52.667777
3228.811848	270100.832345	52.672781
3227.717384	269932.914769	52.677786
3227.249278	269785.221839	52.682791
3226.855047	269626.234796	52.687796
3225.967903	269455.559421	52.692801
3225.034327	269310.588931	52.697805
3224.505910	269145.485370	52.702810
3223.944609	268995.617078	52.707815
3223.047925	268836.913456	52.712820
3222.314606	268683.532364	52.717825
3221.497109	268524.994571	52.722829
3220.958635	268369.494334	52.727834
3220.295182	268233.548051	52.732839
3219.575253	268071.225645	52.737844
3218.804048	267929.999088	52.742849
3217.965948	267780.073020	52.747853
3217.883987	267612.148680	52.752858
3216.980341	267467.836075	52.757863
3216.442829	267317.200408	52.762868
3215.698870	267162.395196	52.767873
3214.881828	267002.609831	52.772877
3214.624331	266852.235619	52.777882
3213.953936	266716.800188	52.782887
3213.297610	266544.331869	52.787892
3212.529884	266394.751635	52.792897
3211.643450	266242.032182	52.797901
3211.260993	266094.224798	52.802906
3210.245689	265934.904124	52.807911
3209.685170	265783.330266	52.812916
3209.257693	265620.733191	52.817921
3208.269123	265475.645129	52.822925
3207.885257	265324.960337	52.827930
3206.780265	265174.542502	52.832935
3206.335013	265020.658558	52.837940
3205.683613	264868.462713	52.842945
3204.726920	264721.026817	52.847949
3204.261447	264555.660166	52.852954
3203.945079	264418.437631	52.857959
3203.205578	264260.143640	52.862964
3202.630368	264112.647625	52.867969
3201.846673	263942.721884	52.872973
3201.167920	263798.680558	52.877978
3199.990851	263650.032026	52.882983
3199.427567	263489.520247	52.887988
3199.057000	263340.744244	52.892993
3198.137559	263202.344195	52.897997
3197.652759	263056.871754	52.903002
3197.263088	262908.124432	52.908007
3196.484660	262760.457402	52.913012
3196.135183	262596.092035	52.918017
3195.309002	262447.846941	52.923021
3194.620424	262281.650765	52.928026
3193.902683	262149.586219	52.933031
3193.010806	261987.089737	52.938036
3192.469214	261835.896572	52.943041
3191.408335	261686.135439	52.948045
3191.087987	261534.881951	52.953050
3190.347754	261384.739155	52.958055
3189.626846	261241.164065	52.963060
3188.861443	261088.300351	52.968065
3188.309162	260943.272533	52.973069
3187.415719	260784.469786	52.978074
3186.858194	260656.200719	52.983079
3186.149332	260493.777982	52.988084
3186.053462	260346.997388	52.993089
3185.086291	260216.934199	52.998093
3184.319744	260051.388326	53.003098
3183.693980	259905.812391	53.008103
3183.074896	259755.778641	53.013108
3182.537927	259605.197164	53.018113
3181.843257	259458.409934	53.023117
3181.341118	259310.395346	53.028122
3180.413481	259155.699259	53.033127
3179.660880	259013.709356	53.038132
3179.752279	258846.016565	53.043137
3178.140131	258718.730275	53.048141
3177.598984	258546.222537	53.053146
3177.394464	258403.127563	53.058151
3176.565860	258252.465705	53.063156
3175.869711	258096.027334	53.068161
3175.193503	257959.679737	53.073165
3174.521010	257801.989912	53.078170
3173.501927	257651.384044	53.083175
3172.831516	257508.159589	53.088180
3172.535618	257362.074550	53.093185
3171.716170	257208.279427	53.098189
3171.336539	257065.212979	53.103194
3170.566107	256912.607269	53.108199
3169.958040	256761.707751	53.113204
3169.240971	256620.681433	53.118209
3168.217897	256474.304560	53.123213
3167.747949	256320.989566	53.128218
3167.392676	256178.760260	53.133223
3166.700351	256024.156368	53.138228
3166.068170	255875.247729	53.143233
3165.362364	255727.878878	53.148237
3164.613176	255568.292746	53.153242
3163.969378	255422.544200	53.158247
3163.385994	255267.618024	53.163252
3162.201561	255116.225134	53.168257
3161.648129	254981.311601	53.173261
3161.138731	254814.888397	53.178266
3160.291634	254674.189576	53.183271
3159.608407	254520.323924	53.188276
3159.422144	254376.031762	53.193281
3158.546978	254237.018519	53.198285
3157.787036	254080.593184	53.203290
3157.329345	253939.578604	53.208295
3156.482871	253792.946516	53.213300
3155.804601	253638.520509	53.218305
3155.148204	253510.678630	53.223309
3154.475332	253348.713799	53.228314
3153.844567	253207.192348	53.233319
3152.799661	253053.232311	53.238324
3152.333962	252913.696848	53.243329
3151.573169	252772.450976	53.248333
3150.958935	252626.648932	53.253338
3150.545000	252482.241452	53.258343
3149.707657	252335.048810	53.263348
3148.988947	252188.525120	53.268353
3148.202126	252048.404474	53.273357
3147.914751	251895.802629	53.278362
3147.191351	251755.774048	53.283367
3146.269450	251615.420459	53.288372
3145.977643	251471.427416	53.293377
3145.285187	251315.961519	53.298381
3144.276940	251178.856210	53.303386
3143.601486	251045.416469	53.308391
3143.197724	250896.322849	53.313396
3142.486713	250738.823096	53.318401
3141.677753	250607.798684	53.323405
3141.239682	250448.473361	53.328410
3140.401783	250317.937622	53.333415
3139.762514	250174.331740	53.338420
3139.303274	250026.979402	53.343425
3138.312846	249880.551645	53.348429
3137.780256	249733.720510	53.353434
3137.343279	249596.016795	53.358439
3136.781462	249448.222826	53.363444
3136.173435	249303.823325	53.368449
3134.987663	249161.145224	53.373453
3134.631726	249010.033939	53.378458
3134.165855	248870.247200	53.383463
3133.317038	248721.760814	53.388468
3132.583801	248576.032095	53.393473
3131.921511	248430.292288	53.398477
3131.346174	248281.024535	53.403482
3130.160164	248142.549329	53.408487
3130.186405	247995.656873	53.413492
3129.344817	247853.231121	53.418497
3128.398868	247701.756114	53.423501
3127.830644	247559.338317	53.428506
3127.307020	247405.912298	53.433511
3126.564037	247275.007587	53.438516
3126.007469	247128.768471	53.443521
3124.927287	247000.973281	53.448525
3124.299780	246844.075465	53.453530
3123.690488	246711.749485	53.458535
3122.885097	246571.738514	53.463540
3122.477548	246420.332440	53.468545
3121.669918	246296.925798	53.473549
3121.180473	246145.176459	53.478554
3120.378881	246015.148014	53.483559
3119.602675	245862.374801	53.488564
3119.187422	245718.890537	53.493569
3118.557281	245590.541558	53.498573
3117.963533	245432.825075	53.503578
3117.286775	245296.563941	53.508583
3116.435178	245147.445034	53.513588
3116.140129	244996.557490	53.518593
3114.895012	244869.936307	53.523597
3114.686136	244722.345951	53.528602
3113.693181	244588.223742	53.533607
3113.058341	244448.187945	53.538612
3112.424812	244294.859147	53.543617
3111.573429	244167.463293	53.548621
3110.995961	244031.009479	53.553626
3110.315863	243897.984404	53.558631
3109.909905	243756.181482	53.563636
3109.375826	243606.784874	53.568641
3108.600364	243472.476599	53.573645
3108.058444	243323.030631	53.578650
3107.457489	243181.972227	53.583655
3106.557826	243056.775117	53.588660
3106.180918	242903.025381	53.593665
3105.427833	242761.864195	53.598669
3104.879431	242607.810914	53.603674
3103.595181	242468.389350	53.608679
3102.904398	242336.538992	53.613684
3102.637302	242194.257471	53.618689
3101.866674	242054.576834	53.623693
3100.987997	241908.954662	53.628698
3100.616547	241784.668371	53.633703
3099.830051	241635.746964	53.638708
3099.315874	241500.253544	53.643713
3098.308188	241355.340004	53.648717
3098.485449	241217.802148	53.653722
3097.276038	241076.307686	53.658727
3096.485117	240944.805727	53.663732
3096.146210	240790.084970	53.668737
3094.982748	240657.547307	53.673741
3094.430473	240508.182803	53.678746
3093.948566	240381.012483	53.683751
3093.002640	240229.928112	53.688756
3092.568391	240090.247463	53.693761
3091.510082	239962.430352	53.698765
3091.071507	239824.915192	53.703770
3090.209510	239685.557374	53.708775
3089.725235	239546.292733	53.713780
3089.163630	239416.131287	53.718785
3088.486957	239286.904918	53.723789
3087.816256	239150.522275	53.728794
3087.083685	239007.987227	53.733799
3086.336274	238872.864810	53.738804
3085.937790	238736.210408	53.743809
3085.365728	238606.840943	53.748813
3084.739135	238453.289292	53.753818
3083.984987	238323.999903	53.758823
3083.158077	238182.448479	53.763828
3082.845777	238034.602558	53.768833
3081.749217	237900.784325	53.773837
3081.089245	237757.628259	53.778842
3080.610810	237626.539040	53.783847
3079.904074	237490.164147	53.788852
3079.433769	237351.791285	53.793857
3078.477715	237222.509694	53.798861
3077.900189	237078.857666	53.803866
3077.058407	236933.516114	53.808871
3076.513058	236812.114730	53.813876
3075.766827	236676.561965	53.818881
3075.060405	236535.986722	53.823885
3074.399407	236410.147952	53.828890
3073.866660	236277.210138	53.833895
3073.277002	236133.128432	53.838900
3072.621794	235981.571006	53.843905
3071.987432	235853.717067	53.848909
3071.105301	235716.175437	53.853914
3070.686568	235571.965604	53.858919
3070.050715	235443.246652	53.863924
3069.321922	235294.528325	53.868929
3068.541634	235168.557165	53.873933
3068.173741	235036.537003	53.878938
3067.586331	234892.864093	53.883943
3066.588633	234760.230999	53.888948
3066.075577	234619.500451	53.893953
3065.330638	234483.975833	53.898957
3064.715449	234339.696994	53.903962
3063.813641	234206.922140	53.908967
3063.086528	234067.652185	53.913972
3062.797985	233933.532942	53.918977
3061.813414	233793.005507	53.923981
3061.049909	233657.383105	53.928986
3060.786486	233532.325261	53.933991
3060.035651	233397.617881	53.938996
3059.651406	233247.702242	53.944001
3058.772542	233116.656709	53.949005
3058.310979	232970.827794	53.954010
3057.343326	232830.477311	53.959015
3056.693284	232707.034953	53.964020
3056.193803	232562.765885	53.969025
3055.514944	232425.833215	53.974029
3054.623283	232278.418354	53.979034
3053.676614	232150.287616	53.984039
3053.006342	232017.326342	53.989044
3053.086282	231877.702643	53.994049
3052.313000	231749.443157	53.999053
3051.521742	231615.763187	54.004058
3051.162858	231476.464166	54.009063
3050.116951	231337.936117	54.014068
3049.741997	231199.123840	54.019073
3048.681098	231058.205122	54.024077
3048.092384	230922.940891	54.029082
3047.700792	230798.670805	54.034087
3046.714111	230647.708850	54.039092
3046.225323	230506.776811	54.044097
3045.260314	230372.616902	54.049101
3044.611474	230248.082738	54.054106
3044.243916	230105.629870	54.059111
3043.352225	229972.833899	54.064116
3042.934132	229825.933621	54.069121
3041.730519	229699.094602	54.074125
3041.241685	229571.455154	54.079130
3040.627842	229441.034873	54.084135
3039.800705	229309.706456	54.089140
3039.625665	229162.616027	54.094145
3038.862271	229033.951415	54.099149
3038.242827	228896.963694	54.104154
3037.641856	228758.369177	54.109159
3036.810717	228626.227639	54.114164
3036.157373	228491.002769	54.119169
3035.351604	228360.003389	54.124173
3034.887659	228216.677658	54.129178
3034.328480	228090.782875	54.134183
3033.333766	227954.670801	54.139188
3032.944672	227802.829795	54.144193
3032.144678	227662.486234	54.149197
3031.220644	227525.447045	54.154202
3030.588265	227385.510250	54.159207
3030.013258	227262.903688	54.164212
3029.742617	227128.180529	54.169217
3028.876031	227003.354451	54.174221
3028.201130	226860.038923	54.179226
3027.518704	226728.131380	54.184231
3026.659368	226597.996126	54.189236
3026.282798	226452.966373	54.194241
3025.317739	226327.915008	54.199245
3024.698342	226193.477699	54.204250
3024.121036	226061.210848	54.209255
3023.535426	225930.855083	54.214260
3022.974625	225799.337131	54.219265
3022.043546	225656.751663	54.224269
3021.541628	225515.155128	54.229274
3020.934136	225394.109556	54.234279
3020.158718	225253.702496	54.239284
3019.531335	225113.195862	54.244289
3018.775221	224974.326591	54.249293
3017.959620	224845.842116	54.254298
3017.408997	224724.062917	54.259303
3016.992427	224597.616159	54.264308
3016.344767	224453.320282	54.269313
3015.576777	224321.799326	54.274317
3014.896301	224180.768054	54.279322
3013.939779	224051.708841	54.284327
3013.292834	223925.821545	54.289332
3012.665786	223799.307526	54.294337
3011.922648	223677.891376	54.299341
3011.182643	223542.942894	54.304346
3010.892364	223404.142642	54.309351
3009.986759	223268.940784	54.314356
3009.422373	223136.676686	54.319361
3008.875673	223026.598305	54.324365
3008.306250	222876.857231	54.329370
3007.358469	222737.143848	54.334375
3006.680735	222614.636952	54.339380
3006.106659	222471.962479	54.344385
3005.631482	222338.934556	54.349389
3005.071755	222220.992343	54.354394
3004.186785	222082.848698	54.359399
3003.355740	221963.473175	54.364404
3002.672207	221823.414106	54.369409
3001.945117	221700.381831	54.374413
3001.539775	221570.195646	54.379418
3000.842276	221431.221534	54.384423
3000.122719	221316.883061	54.389428
2999.756899	221188.358862	54.394433
2998.589466	221059.452592	54.399437
2998.229254	220929.973225	54.404442
2997.601808	220793.509659	54.409447
2996.973466	220665.944440	54.414452
2995.895910	220530.240003	54.419457
2995.373681	220410.805322	54.424461
2995.155283	220273.666937	54.429466
2994.439473	220143.659669	54.434471
2993.215457	220018.939422	54.439476
2992.965883	219890.119008	54.444481
2992.336861	219764.248461	54.449485
2991.482774	219625.913512	54.454490
2991.045310	219491.089819	54.459495
2990.197306	219354.854762	54.464500
2989.858513	219228.124515	54.469505
2989.018787	219093.798032	54.474509
2988.217122	218968.363524	54.479514
2987.628470	218829.708024	54.484519
2986.634889	218711.292693	54.489524
2986.127468	218576.392668	54.494529
2985.617007	218447.985252	54.499533
2984.711134	218317.871311	54.504538
2984.017955	218183.803366	54.509543
2983.249904	218063.991386	54.514548
2982.775248	217944.133161	54.519553
2982.014892	217816.441081	54.524557
2981.365778	217691.595653	54.529562
2980.579945	217552.922927	54.534567
2980.366066	217434.729967	54.539572
2979.625959	217310.281487	54.544577
2979.130035	217191.280745	54.549581
2978.349804	217056.070383	54.554586
2977.622364	216918.726200	54.559591
2976.614313	216787.829331	54.564596
2976.480106	216654.401347	54.569601
2975.757295	216538.938066	54.574605
2974.854182	216406.637860	54.579610
2974.790623	216277.285361	54.584615
2973.786960	216152.333335	54.589620
2973.166625	216005.923860	54.594625
2972.414093	215882.790960	54.599629
2971.758739	215748.021613	54.604634
2971.217080	215632.454800	54.609639
2970.548601	215500.004635	54.614644
2969.818166	215363.504110	54.619649
2969.005486	215235.494114	54.624653
2968.406251	215105.490371	54.629658
2967.906363	214968.088601	54.634663
2966.794401	214849.749485	54.639668
2966.161049	214711.822039	54.644673
2965.403228	214593.630965	54.649677
2964.997259	214458.951982	54.654682
2964.200836	214328.955498	54.659687
2963.427241	214208.947436	54.664692
2963.260846	214077.871611	54.669697
2962.355221	213962.072527	54.674701
2961.735322	213832.672753	54.679706
2961.156830	213694.522339	54.684711
2960.254107	213579.372608	54.689716
2959.976673	213435.141875	54.694721
2958.967874	213307.484824	54.699725
2958.225133	213185.971801	54.704730
2957.630606	213057.078658	54.709735
2957.061279	212932.063862	54.714740
2956.445120	212797.039691	54.719745
2955.544323	212673.376135	54.724749
2954.627039	212552.731977	54.729754
2954.527582	212425.709096	54.734759
2953.617245	212300.202195	54.739764
2953.218417	212179.247546	54.744769
2952.500756	212051.801423	54.749773
2951.950990	211920.408765	54.754778
2951.348085	211790.450314	54.759783
2950.474148	211675.732143	54.764788
2949.813916	211531.591690	54.769793
2949.275549	211405.543986	54.774797
2948.493529	211274.596712	54.779802
2948.031585	211145.113641	54.784807
2946.995798	211020.838246	54.789812
2946.456923	210883.654862	54.794817
2945.542470	210766.984671	54.799821
2944.839762	210638.291688	54.804826
2944.159901	210511.389951	54.809831
2943.444054	210386.925146	54.814836
2943.297988	210265.272274	54.819841
2942.447130	210145.169440	54.824845
2941.713407	210023.330070	54.829850
2941.096526	209893.288632	54.834855
2940.424372	209764.783517	54.839860
2939.676762	209638.899750	54.844865
2939.003811	209514.124433	54.849869
2937.948832	209390.173498	54.854874
2937.602940	209263.781430	54.859879
2936.890375	209150.722335	54.864884
2936.614420	209020.666932	54.869889
2935.917334	208906.129462	54.874893
2935.116982	208770.455768	54.879898
2934.829543	208646.512083	54.884903
2933.936942	208523.224460	54.889908
2933.167424	208397.333972	54.894913
2932.448780	208264.028458	54.899917
2931.837652	208137.897067	54.904922
2931.435710	208010.485557	54.909927
2930.558894	207892.185757	54.914932
2930.166538	207749.628003	54.919937
2929.214999	207624.697016	54.924941
2928.265048	207509.922216	54.929946
2927.840330	207381.268390	54.934951
2926.958114	207249.225533	54.939956
2926.562710	207126.994739	54.944961
2925.732645	207009.452893	54.949965
2925.045782	206877.010847	54.954970
2924.511329	206748.973919	54.959975
2923.686806	206643.764266	54.964980
2923.288860	206507.204704	54.969985
2922.882962	206385.206177	54.974989
2921.781351	206262.465360	54.979994
2921.363622	206132.044102	54.984999
2920.520044	206013.068248	54.990004
2919.900740	205868.043761	54.995009
2919.349094	205749.149486	55.000013
2918.795560	205622.454321	55.005018
2918.055461	205499.199701	55.010023
2916.960826	205385.406423	55.015028
2916.560719	205244.001307	55.020033
2915.834275	205122.667031	55.025037
2915.380905	205004.242321	55.030042
2914.270353	204880.716778	55.035047
2913.586575	204765.663374	55.040052
2913.256032	204641.862121	55.045057
2912.241433	204519.811149	55.050061
2911.533638	204390.966883	55.055066
2911.209641	204274.826656	55.060071
2910.298078	204155.432676	55.065076
2910.105612	204035.148782	55.070081
2909.276906	203911.326170	55.075085
2908.589354	203792.622875	55.080090
2908.133868	203663.014901	55.085095
2907.166078	203535.359088	55.090100
2906.800301	203409.758959	55.095105
2905.924361	203306.714223	55.100109
2905.198477	203172.708764	55.105114
2904.690076	203044.866782	55.110119
2903.534643	202929.255457	55.115124
2903.318256	202801.316886	55.120129
2902.387958	202693.458719	55.125133
2901.440998	202556.270057	55.130138
2901.168167	202445.470375	55.135143
2900.502054	202335.763984	55.140148
2899.948983	202200.346357	55.145153
2899.053563	202087.991601	55.150157
2898.484003	201967.530028	55.155162
2898.063763	201837.284388	55.160167
2896.790243	201727.522664	55.165172
2896.037159	201612.855694	55.170177
2895.709774	201496.899887	55.175181
2895.152947	201382.265949	55.180186
2894.711452	201255.384626	55.185191
2893.594731	201150.269540	55.190196
2893.637416	201020.690611	55.195201
2892.709128	200892.958235	55.200205
2891.990722	200770.957597	55.205210
2891.766626	200649.718844	55.210215
2890.761438	200526.224375	55.215220
2890.014437	200391.732681	55.220225
2889.318985	200276.384931	55.225229
2888.624573	200150.055236	55.230234
2888.043663	200023.656962	55.235239
2887.133653	199912.836016	55.240244
2886.973365	199781.510622	55.245249
2886.138548	199665.931733	55.250253
2885.292442	199538.609465	55.255258
2884.830056	199408.936196	55.260263
2884.107286	199293.620320	55.265268
2883.483080	199172.002850	55.270273
2882.430522	199050.122631	55.275277
2881.825711	198928.617169	55.280282
2881.546467	198816.947824	55.285287
2880.143905	198703.471478	55.290292
2879.814761	198578.334696	55.295297
2879.082640	198460.922472	55.300301
2878.423474	198355.931256	55.305306
2878.027389	198223.705374	55.310311
2877.153595	198117.717897	55.315316
2876.647077	197985.331949	55.320321
2876.101302	197872.281610	55.325325
2875.145720	197750.350850	55.330330
2874.763331	197630.009281	55.335335
2873.945894	197518.962340	55.340340
2873.142762	197391.892913	55.345345
2872.474861	197285.759989	55.350349
2871.787578	197166.969281	55.355354
2871.407861	197041.971405	55.360359
2870.519393	196933.825455	55.365364
2869.872916	196808.425019	55.370369
2869.338998	196696.902297	55.375373
2868.747151	196574.674919	55.380378
2868.144278	196454.103763	55.385383
2867.247226	196338.300257	55.390388
2866.930797	196218.422312	55.395393
2866.060029	196095.425872	55.400397
2864.982748	195971.711689	55.405402
2864.536551	195852.135083	55.410407
2863.675130	195746.990287	55.415412
2863.004990	195630.528952	55.420417
2862.596655	195526.356255	55.425421
2861.910584	195409.579838	55.430426
2861.223631	195286.619854	55.435431
2860.243439	195180.197163	55.440436
2859.887214	195055.416701	55.445441
2859.202997	194942.127486	55.450445
2858.202783	194832.196834	55.455450
2857.677273	194712.406427	55.460455
2857.128943	194600.852380	55.465460
2856.667223	194484.144358	55.470465
2855.825019	194379.444693	55.475469
2855.253495	194261.024112	55.480474
2854.678303	194154.437656	55.485479
2854.288870	194043.623117	55.490484
2853.633557	193912.301856	55.495489
2853.342448	193795.517519	55.500493
2852.177691	193672.802543	55.505498
2851.621969	193553.045132	55.510503
2851.314696	193432.536133	55.515508
2850.544931	193305.942383	55.520513
2849.634370	193184.460729	55.525517
2849.115889	193074.775739	55.530522
2848.360655	192942.493136	55.535527
2847.435833	192831.982379	55.540532
2846.933246	192703.248463	55.545537
2846.451039	192576.878234	55.550541
2845.476576	192463.208004	55.555546
2844.670790	192351.737934	55.560551
2843.919324	192230.093477	55.565556
2843.688772	192107.514360	55.570561
2842.893790	191997.252109	55.575565
2842.252310	191877.054302	55.580570
2841.844655	191751.895834	55.585575
2840.768485	191648.142352	55.590580
2839.999102	191527.342220	55.595585
2839.125331	191416.712062	55.600589
2838.533718	191298.123638	55.605594
2837.816070	191186.756781	55.610599
2837.160188	191077.759627	55.615604
2836.885240	190952.862110	55.620609
2836.266774	190847.383854	55.625613
2835.760969	190743.669215	55.630618
2835.173790	190612.116973	55.635623
2834.171628	190504.804501	55.640628
2833.571049	190383.535191	55.645633
2833.161162	190256.790572	55.650637
2832.194911	190147.768339	55.655642
2831.697335	190022.832157	55.660647
2830.856355	189905.877013	55.665652
2830.325879	189782.511578	55.670657
2829.460857	189680.052074	55.675661
2828.753449	189562.656768	55.680666
2828.349408	189433.979551	55.685671
2827.325397	189324.739342	55.690676
2826.842562	189212.614696	55.695681
2826.056521	189110.919996	55.700685
2825.415198	188996.263714	55.705690
2824.724571	188869.783536	55.710695
2824.083206	188762.099795	55.715700
2823.773690	188650.127152	55.720705
2822.782230	188539.280573	55.725709
2822.105540	188419.923982	55.730714
2821.765983	188303.313232	55.735719
2820.961713	188206.712339	55.740724
2820.285962	188085.320871	55.745729
2819.541295	187954.233508	55.750733
2818.862889	187843.148166	55.755738
2818.177553	187728.145732	55.760743
2817.538165	187616.265972	55.765748
2817.012373	187496.557068	55.770753
2816.281914	187391.625866	55.775757
2815.141705	187272.371068	55.780762
2814.857703	187158.146147	55.785767
2813.926585	187051.911676	55.790772
2813.637558	186939.036632	55.795777
2812.834651	186825.403597	55.800781
2812.202255	186706.108005	55.805786
2811.425533	186592.942111	55.810791
2810.870629	186493.557359	55.815796
2810.420006	186372.859878	55.820801
2809.580525	186262.007400	55.825805
2808.726202	186149.198382	55.830810
2808.404842	186032.666804	55.835815
2807.504770	185927.116998	55.840820
2806.895637	185817.132364	55.845825
2806.178074	185700.906096	55.850829
2805.772293	185581.259506	55.855834
2805.023687	185477.595004	55.860839
2804.252831	185367.522577	55.865844
2803.717528	185237.236711	55.870849
2802.887133	185132.122974	55.875853
2801.989661	185018.305878	55.880858
2801.463009	184910.663859	55.885863
2801.126272	184807.431800	55.890868
2800.724236	184679.632560	55.895873
2799.733242	184564.597448	55.900877
2798.790500	184455.457690	55.905882
2798.562204	184335.264718	55.910887
2797.786075	184225.094150	55.915892
2797.071992	184111.199424	55.920897
2796.372499	183999.656101	55.925901
2795.631616	183889.391731	55.930906
2795.065814	183761.493838	55.935911
2794.485498	183660.605530	55.940916
2793.512244	183545.722888	55.945921
2792.870208	183426.144902	55.950925
2792.565713	183318.611462	55.955930
2791.996570	183205.828269	55.960935
2791.055051	183101.194869	55.965940
2790.574185	182976.287934	55.970945
2789.983081	182862.313331	55.975949
2788.994602	182756.136240	55.980954
2788.693127	182627.118487	55.985959
2787.752839	182515.642485	55.990964
2787.074906	182404.112492	55.995969
2786.315198	182287.978114	56.000973
2785.771601	182179.162372	56.005978
2785.045395	182063.684758	56.010983
2784.283791	181958.593085	56.015988
2783.758586	181843.236866	56.020993
2782.937906	181727.368048	56.025997
2782.346594	181620.036843	56.031002
2781.935367	181501.877681	56.036007
2781.290503	181400.470529	56.041012
2780.471584	181283.839388	56.046017
2779.739611	181167.118467	56.051021
2779.146859	181050.083243	56.056026
2778.606265	180932.378617	56.061031
2777.736962	180829.431033	56.066036
2777.334691	180712.773602	56.071041
2776.593178	180598.625223	56.076045
2775.651348	180493.387570	56.081050
2775.442483	180379.562453	56.086055
2774.606796	180264.577628	56.091060
2773.671997	180141.188110	56.096065
2773.057339	180042.972113	56.101069
2772.342973	179933.489468	56.106074
2772.188258	179811.592787	56.111079
2770.983374	179719.487577	56.116084
2770.513801	179590.759899	56.121089
2769.784711	179471.015796	56.126093
2769.367283	179367.338724	56.131098
2768.719023	179248.612754	56.136103
2768.177944	179142.373693	56.141108
2767.447734	179024.348201	56.146113
2766.291829	178913.882382	56.151117
2765.840824	178805.314912	56.156122
2765.885451	178689.151898	56.161127
2764.881874	178576.055307	56.166132
2763.953773	178452.656922	56.171137
2763.319394	178339.896795	56.176141
2762.362393	178245.262507	56.181146
2761.786143	178130.305978	56.186151
2761.065368	178012.459903	56.191156
2760.449645	177895.271649	56.196161
2760.108415	177785.875383	56.201165
2759.141469	177678.142994	56.206170
2758.672475	177554.254798	56.211175
2757.893545	177447.459893	56.216180
2757.157444	177336.575601	56.221185
2756.570646	177225.731551	56.226189
2755.921654	177123.890107	56.231194
2755.156825	177008.292427	56.236199
2754.564311	176906.124594	56.241204
2753.851908	176781.297889	56.246209
2753.483310	176672.036080	56.251213
2752.682788	176559.777697	56.256218
2752.228814	176450.148430	56.261223
2751.043510	176347.465367	56.266228
2750.900001	176224.941394	56.271233
2749.866488	176112.263258	56.276237
2748.948336	176008.432186	56.281242
2748.554952	175899.774140	56.286247
2747.911075	175788.993869	56.291252
2747.237782	175685.188425	56.296257
2746.352386	175581.264218	56.301261
2745.955838	175482.426621	56.306266
2745.582247	175358.835159	56.311271
2744.529039	175252.877953	56.316276
2744.194763	175133.020217	56.321281
2743.404194	175016.427463	56.326285
2742.650699	174909.469788	56.331290
2742.346729	174792.584384	56.336295
2741.660460	174692.192076	56.341300
2741.012366	174572.818132	56.346305
2740.079025	174462.646938	56.351309
2739.446697	174346.972205	56.356314
2738.967773	174225.092421	56.361319
2738.034767	174116.944326	56.366324
2737.261048	174008.720417	56.371329
2736.715055	173904.505106	56.376333
2736.197976	173790.950370	56.381338
2735.822014	173677.895043	56.386343
2735.073386	173566.768625	56.391348
2734.183902	173457.890483	56.396353
2733.248029	173343.487658	56.401357
2732.314995	173234.820512	56.406362
2732.099611	173121.614143	56.411367
2731.220160	173017.619299	56.416372
2730.502329	172904.989135	56.421377
2730.219572	172796.118435	56.426381
2729.200742	172697.170051	56.431386
2728.646197	172578.397690	56.436391
2727.836929	172473.998904	56.441396
2727.443720	172367.067254	56.446401
2726.910689	172262.078408	56.451405
2726.134882	172155.246092	56.456410
2725.809427	172035.269051	56.461415
2724.713724	171925.652012	56.466420
2724.053652	171821.434800	56.471425
2723.646579	171702.946931	56.476429
2722.854163	171593.740604	56.481434
2722.196889	171476.526645	56.486439
2721.391252	171379.849647	56.491444
2720.932083	171260.735499	56.496449
2720.464983	171153.640810	56.501453
2719.483934	171045.813926	56.506458
2718.940299	170928.125788	56.511463
2718.286446	170815.160822	56.516468
2717.712337	170706.685421	56.521473
2716.810935	170596.634381	56.526477
2716.331067	170488.233681	56.531482
2715.816219	170373.314983	56.536487
2715.058724	170265.785492	56.541492
2714.363557	170140.264636	56.546497
2714.220867	170027.246421	56.551501
2712.921710	169924.686985	56.556506
2712.174958	169805.292215	56.561511
2711.885816	169697.397623	56.566516
2711.474135	169581.574758	56.571521
2710.464106	169467.016969	56.576525
2710.159613	169360.461011	56.581530
2709.469957	169229.766547	56.586535
2708.713191	169124.325658	56.591540
2707.887563	168997.926313	56.596545
2707.333064	168889.262166	56.601549
2706.331841	168775.824106	56.606554
2705.569576	168666.214336	56.611559
2705.294217	168554.378668	56.616564
2704.398025	168432.811902	56.621569
2703.728465	168317.453354	56.626573
2702.946240	168205.533695	56.631578
2702.440821	168094.587817	56.636583
2701.356280	167994.682699	56.641588
2700.994857	167877.318371	56.646593
2700.757778	167767.017616	56.651597
2699.635644	167654.555773	56.656602
2699.054439	167531.911988	56.661607
2698.419193	167418.483588	56.666612
2697.718301	167325.589591	56.671617
2697.237184	167203.541387	56.676621
2696.503737	167097.339476	56.681626
2695.918177	166977.559275	56.686631
2694.939464	166873.380534	56.691636
2694.736421	166753.502301	56.696641
2694.056838	166636.497419	56.701645
2692.787756	166529.402858	56.706650
2692.471258	166413.549149	56.711655
2691.602597	166306.162909	56.716660
2691.053674	166200.442936	56.721665
2690.484238	166080.078132	56.726669
2689.953522	165976.848168	56.731674
2689.332951	165862.557496	56.736679
2688.370942	165755.073194	56.741684
2687.555390	165641.805901	56.746689
2687.272998	165528.797802	56.751693
2686.115869	165435.090709	56.756698
2686.260190	165317.616129	56.761703
2685.615835	165215.588813	56.766708
2684.943962	165098.256952	56.771713
2683.868467	164985.503315	56.776717
2682.877539	164866.150157	56.781722
2682.850547	164750.166768	56.786727
2682.333974	164649.989900	56.791732
2681.455783	164533.976749	56.796737
2680.983631	164409.723871	56.801741
2679.972669	164295.080305	56.806746
2679.460032	164180.815886	56.811751
2678.884154	164065.913383	56.816756
2678.139350	163944.515275	56.821761
2677.415341	163839.846992	56.826765
2676.286884	163731.021775	56.831770
2676.132428	163614.629869	56.836775
2675.575924	163502.968331	56.841780
2674.873856	163385.748455	56.846785
2674.096717	163278.305691	56.851789
2673.425011	163155.182157	56.856794
2672.747021	163043.464992	56.861799
2672.036110	162928.396755	56.866804
2671.399204	162810.812407	56.871809
2670.964084	162706.928061	56.876813
2669.868555	162595.901438	56.881818
2669.692539	162471.481115	56.886823
2668.672195	162363.049740	56.891828
2668.090382	162247.200362	56.896833
2667.583760	162135.802140	56.901837
2666.976277	162029.416923	56.906842
2666.461459	161911.027889	56.911847
2665.754664	161795.415909	56.916852
2665.184593	161670.564939	56.921857
2664.446891	161559.205119	56.926861
2663.403570	161444.944421	56.931866
2662.923393	161334.218343	56.936871
2662.335472	161218.271547	56.941876
2661.609791	161094.985626	56.946881
2660.975105	160984.145262	56.951885
2660.296590	160869.574335	56.956890
2660.046434	160741.027075	56.961895
2659.199404	160621.258301	56.966900
2658.569222	160509.249045	56.971905
2657.923781	160392.182543	56.976909
2656.837049	160287.416804	56.981914
2656.547881	160150.982734	56.986919
2655.783668	160041.043075	56.991924
2654.625241	159922.813483	56.996929
2654.322948	159811.911411	57.001933
2653.686547	159689.951145	57.006938
2652.981905	159581.211252	57.011943
2652.143855	159468.577143	57.016948
2651.627883	159350.158694	57.021953
2650.991570	159237.480650	57.026957
2650.240563	159123.867654	57.031962
2649.765549	159003.524200	57.036967
2648.853909	158890.954461	57.041972
2648.015247	158774.279926	57.046977
2647.803590	158656.959779	57.051981
2647.177887	158555.164573	57.056986
2646.535204	158428.378777	57.061991
2645.644964	158326.003223	57.066996
2645.070225	158207.750513	57.072001
2644.480406	158092.310120	57.077005
2643.384523	157982.175230	57.082010
2643.157714	157859.647949	57.087015
2642.335943	157747.499906	57.092020
2641.539852	157639.657735	57.097025
2640.975231	157522.384633	57.102029
2640.319153	157405.927309	57.107034
2639.696341	157292.922905	57.112039
2639.025225	157189.867658	57.117044
2638.650289	157068.243813	57.122049
2638.062273	156950.747540	57.127053
2637.274212	156847.063521	57.132058
2636.673508	156719.997669	57.137063
2635.905569	156603.370104	57.142068
2635.510926	156480.314981	57.147073
2634.841293	156360.647166	57.152077
2633.744591	156241.238119	57.157082
2633.313278	156119.906238	57.162087
2632.583936	156009.325522	57.167092
2631.918761	155886.684051	57.172097
2631.332499	155772.216997	57.177101
2630.644446	155663.588499	57.182106
2629.954857	155544.142815	57.187111
2629.202112	155421.466051	57.192116
2628.768380	155310.713651	57.197121
2628.011496	155189.309558	57.202125
2627.126654	155071.447306	57.207130
2626.909992	154942.369640	57.212135
2626.220564	154838.993900	57.217140
2625.386310	154707.739617	57.222145
2624.998289	154592.240930	57.227149
2624.418432	154474.383284	57.232154
2623.487852	154344.467670	57.237159
2622.642212	154232.373112	57.242164
2622.009252	154117.982616	57.247169
2621.272732	154003.354695	57.252173
2620.851755	153890.227936	57.257178
2620.008044	153755.203644	57.262183
2619.524599	153646.574647	57.267188
2618.859821	153533.462303	57.272193
2618.346780	153398.310790	57.277197
2617.348183	153285.747912	57.282202
2616.886410	153170.596296	57.287207
2616.330508	153045.303987	57.292212
2615.525432	152923.788623	57.297217
2615.016647	152803.497834	57.302221
2614.414265	152682.281717	57.307226
2613.783297	152554.295764	57.312231
2612.812697	152442.570216	57.317236
2611.954052	152319.616540	57.322241
2611.574446	152203.959545	57.327245
2610.774345	152085.598691	57.332250
2610.433871	151956.984336	57.337255
2609.630782	151848.170377	57.342260
2609.016368	151725.192927	57.347265
2608.545825	151601.468650	57.352269
2607.434272	151485.510719	57.357274
2607.301242	151363.131990	57.362279
2606.467063	151239.479409	57.367284
2605.973154	151113.612650	57.372289
2605.399861	150985.954119	57.377293
2604.388002	150864.224916	57.382298
2603.976084	150747.485104	57.387303
2603.508929	150629.928314	57.392308
2602.409308	150488.450435	57.397313
2601.892108	150367.852143	57.402317
2601.057165	150249.795771	57.407322
2600.733406	150118.440670	57.412327
2599.826217	149999.684909	57.417332
2598.736811	149874.705301	57.422337
2598.589901	149749.589535	57.427341
2597.613886	149631.227321	57.432346
2597.352306	149501.453562	57.437351
2596.194252	149392.881982	57.442356
2595.759004	149268.970328	57.447361
2595.154212	149148.428585	57.452365
2594.487541	149021.491593	57.457370
2593.939287	148901.678955	57.462375
2593.190704	148782.432297	57.467380
2592.417104	148667.295114	57.472385
2592.158495	148492.979259	57.477389
2591.217023	148366.800112	57.482394
2590.877204	148236.039838	57.487399
2590.266721	148099.121011	57.492404
2589.541802	147974.726478	57.497409
2588.838488	147844.521054	57.502413
2588.076278	147728.444991	57.507418
2588.042670	147587.548046	57.512423
2587.108567	147452.132079	57.517428
2585.495615	147339.420263	57.522433
2585.507932	147219.703019	57.527437
2584.828992	147070.128978	57.532442
2584.224086	146952.976011	57.537447
2583.274542	146840.999602	57.542452
2582.844846	146699.991443	57.547457
2582.091858	146585.023735	57.552461
2581.431253	146456.520160	57.557466
2580.850982	146326.479388	57.562471
2580.269008	146208.410554	57.567476
2578.986873	146077.160383	57.572481
2578.362466	145947.039215	57.577485
2577.559798	145823.516900	57.582490
2577.216495	145711.245109	57.587495
2576.598450	145594.658428	57.592500
2576.018691	145467.632916	57.597505
2575.380207	145343.845023	57.602509
2574.658014	145224.849023	57.607514
2574.136518	145086.543999	57.612519
2573.235425	144959.482521	57.617524
2572.581150	144866.527929	57.622529
2572.422492	144717.975493	57.627533
2571.404284	144603.781419	57.632538
2570.993538	144477.317704	57.637543
2569.894798	144354.356423	57.642548
2569.356166	144221.395092	57.647553
2569.019883	144109.166078	57.652557
2568.446448	143976.999167	57.657562
2567.833142	143845.792183	57.662567
2566.931761	143727.376728	57.667572
2565.828740	143592.182125	57.672577
2565.455574	143459.502819	57.677581
2564.548334	143353.745991	57.682586
2564.204127	143210.363837	57.687591
2563.577594	143085.464851	57.692596
2562.840735	142975.031587	57.697601
2562.389252	142832.112939	57.702605
2561.482180	142734.897208	57.707610
2561.481776	142587.537078	57.712615
2560.376365	142459.793983	57.717620
2559.574444	142329.068097	57.722625
2558.815286	142218.666509	57.727629
2558.329197	142073.761954	57.732634
2557.500660	141953.346882	57.737639
2557.048673	141828.120412	57.742644
2556.132326	141693.705112	57.747649
2555.537760	141564.868303	57.752653
2554.698907	141457.607857	57.757658
2554.306891	141337.278520	57.762663
2553.761734	141206.809007	57.767668
2552.696794	141066.664148	57.772673
2552.220413	140956.527278	57.777677
2551.942765	140822.497450	57.782682
2551.386170	140699.363295	57.787687
2550.279044	140574.360186	57.792692
2549.610772	140447.737933	57.797697
2549.260809	140310.024443	57.802701
2548.476238	140194.424892	57.807706
2548.223515	140065.197245	57.812711
2547.562273	139910.420381	57.817716
2546.558171	139808.960334	57.822721
2545.952601	139665.585510	57.827725
2545.036008	139529.794993	57.832730
2544.372489	139424.800980	57.837735
2543.831400	139283.234641	57.842740
2543.062054	139168.398958	57.847745
2542.833639	139010.496176	57.852749
2541.614166	138891.895919	57.857754
2541.178095	138772.689182	57.862759
2540.352300	138635.160453	57.867764
2539.360236	138519.930597	57.872769
2539.472919	138376.448137	57.877773
2538.823639	138256.184637	57.882778
2537.964492	138129.170496	57.887783
2537.173190	137993.849918	57.892788
2536.283171	137881.719047	57.897793
2536.242013	137735.443618	57.902797
2535.314502	137618.187000	57.907802
2534.774295	137491.620533	57.912807
2534.357455	137342.065291	57.917812
2533.611411	137222.050020	57.922817
2532.483049	137090.052056	57.927821
2531.577521	136960.179108	57.932826
2531.674867	136824.291112	57.937831
2530.740656	136697.218817	57.942836
2530.117523	136564.317371	57.947841
2529.755760	136432.696332	57.952845
2528.708163	136315.400431	57.957850
2528.142585	136162.254119	57.962855
2527.375108	136033.481356	57.967860
2526.571689	135922.258934	57.972865
2526.123070	135775.232100	57.977869
2525.397640	135650.964225	57.982874
2524.972803	135517.337412	57.987879
2524.270667	135383.437572	57.992884
2523.392236	135259.525918	57.997889
2522.954501	135112.919928	58.002893
2521.880139	134996.853131	58.007898
2521.416709	134866.665376	58.012903
2520.984016	134728.698869	58.017908
2520.328205	134597.844130	58.022913
2519.633799	134461.660734	58.027917
2518.613350	134338.397998	58.032922
2518.027354	134197.498484	58.037927
2517.242816	134072.154293	58.042932
2516.421745	133960.256247	58.047937
2516.511571	133816.367896	58.052941
2515.531082	133687.652044	58.057946
2515.033663	133554.579343	58.062951
2514.224661	133411.280085	58.067956
2513.354214	133295.403785	58.072961
2513.326897	133145.084377	58.077965
2511.864533	133027.740552	58.082970
2511.936223	132876.924164	58.087975
2510.963824	132750.396092	58.092980
2510.061842	132627.287082	58.097985
2509.635366	132489.978185	58.102989
2509.278134	132357.231812	58.107994
2508.443157	132219.569792	58.112999
2508.067948	132115.318585	58.118004
2507.462797	131946.602671	58.123009
2506.498390	131823.659468	58.128013
2505.797231	131666.557446	58.133018
2505.146314	131544.683545	58.138023
2504.499409	131396.719836	58.143028
2503.501915	131273.276199	58.148033
2503.790633	131153.312752	58.153037
2502.547316	130991.994516	58.158042
2501.978677	130863.708858	58.163047
2501.385579	130743.086724	58.168052
2500.775696	130580.971859	58.173057
2500.051701	130469.783480	58.178061
2499.390797	130303.042271	58.183066
2498.918583	130174.426947	58.188071
2498.222084	130030.352204	58.193076
2497.174457	129884.746209	58.198081
2496.601079	129768.684882	58.203085
2495.763658	129590.455959	58.208090
2495.504717	129477.737191	58.213095
2494.471336	129342.483108	58.218100
2493.888998	129196.235419	58.223105
2493.357691	129060.865023	58.228109
2492.352095	128932.327275	58.233114
2491.958772	128801.813369	58.238119
2491.194717	128661.338027	58.243124
2490.419317	128531.178073	58.248129
2489.862912	128376.319601	58.253133
2488.977466	128258.421678	58.258138
2488.713120	128086.995235	58.263143
2487.771511	127997.289503	58.268148
2487.099344	127834.590908	58.273153
2487.051523	127716.003724	58.278157
2485.821773	127565.041205	58.283162
2485.395546	127455.024226	58.288167
2484.712351	127289.041284	58.293172
2484.201453	127180.981928	58.298177
2483.724713	127029.928396	58.303181
2483.041847	126881.600734	58.308186
2482.236595	126761.105765	58.313191
2481.245496	126603.240145	58.318196
2480.701889	126487.226005	58.323201
2480.397162	126320.731762	58.328205
2479.193587	126220.901027	58.333210
2478.855231	126071.596095	58.338215
2478.174001	125908.326218	58.343220
2477.650392	125755.153680	58.348225
2477.109630	125659.245627	58.353229
2476.252362	125503.803434	58.358234
2475.859450	125347.742464	58.363239
2474.722330	125238.596366	58.368244
2474.146652	125071.784457	58.373249
2473.677066	124948.107678	58.378253
2472.678856	124808.006736	58.383258
2472.433063	124642.313486	58.388263
2471.551217	124554.806521	58.393268
2470.725492	124401.664147	58.398273
2469.654562	124254.212390	58.403277
2469.411251	124106.033421	58.408282
2469.096978	123945.929970	58.413287
2468.140815	123861.624359	58.418292
2467.408477	123693.969637	58.423297
2467.242572	123571.724059	58.428301
2466.112844	123443.371601	58.433306
2465.438463	123262.339181	58.438311
2464.992553	123168.507468	58.443316
2464.222893	123011.783298	58.448321
2464.105972	122870.359178	58.453325
2462.644621	122724.234849	58.458330
2462.067269	122605.081016	58.463335
2461.365424	122439.435603	58.468340
2460.546863	122321.197426	58.473345
2460.157154	122153.498085	58.478349
2459.132084	122063.647548	58.483354
2458.920709	121915.272529	58.488359
2458.400320	121759.239997	58.493364
2457.605424	121648.949653	58.498369
2457.293866	121534.189883	58.503373
2456.353909	121367.941362	58.508378
2456.010908	121217.038988	58.513383
2455.143970	121097.747397	58.518388
2454.575171	120923.799195	58.523393
2453.853226	120816.192541	58.528397
2453.156793	120658.683497	58.533402
2452.329646	120523.529809	58.538407
2451.870650	120353.935682	58.543412
2451.059822	120255.347407	58.548417
2450.388270	120080.798949	58.553421
2449.500684	119959.090764	58.558426
2449.423347	119802.745688	58.563431
2448.838894	119681.949326	58.568436
2447.982144	119522.917229	58.573441
2447.298058	119386.147011	58.578445
2446.513292	119241.864630	58.583450
2445.913544	119099.248653	58.588455
2445.080669	118961.596485	58.593460
2444.286468	118832.883241	58.598465
2443.644080	118662.980054	58.603469
2443.033207	118535.991259	58.608474
2442.423681	118396.338833	58.613479
2441.722998	118255.381258	58.618484
2441.031255	118118.390423	58.623489
2440.380117	117986.783151	58.628493
2439.884018	117833.474395	58.633498
2439.168733	117695.283468	58.638503
2438.452203	117550.231638	58.643508
2437.831815	117431.450997	58.648513
2437.776138	117256.068563	58.653517
2436.533101	117148.521646	58.658522
2436.076094	116996.652586	58.663527
2435.682467	116850.664864	58.668532
2434.330607	116719.225954	58.673537
2434.117873	116554.244997	58.678541
2433.304207	116413.251972	58.683546
2432.580562	116296.543176	58.688551
2432.332285	116133.531910	58.693556
2431.390358	115991.837953	58.698561
2431.308370	115846.955426	58.703565
2430.267010	115692.133734	58.708570
2429.557288	115559.361305	58.713575
2428.940873	115409.627885	58.718580
2427.971702	115251.738111	58.723585
2427.581937	115119.951839	58.728589
2426.696484	114970.892024	58.733594
2426.022828	114826.642274	58.738599
2425.481389	114667.114284	58.743604
2425.015653	114536.047612	58.748609
2424.481716	114395.167438	58.753613
2423.446383	114243.184378	58.758618
2422.899879	114099.477154	58.763623
2422.398892	113963.075030	58.768628
2421.618935	113803.641097	58.773633
2421.489291	113656.595397	58.778637
2420.659581	113516.293816	58.783642
2419.838526	113371.637856	58.788647
2419.411649	113219.862824	58.793652
2418.517218	113058.249513	58.798657
2417.583326	112898.299945	58.803661
2416.868374	112766.069844	58.808666
2416.526687	112624.636037	58.813671
2415.596691	112469.435746	58.818676
2414.453890	112323.504127	58.823681
2414.069445	112193.109543	58.828685
2413.704684	112026.018224	58.833690
2413.032861	111894.737862	58.838695
2412.253250	111770.506904	58.843700
2411.786124	111594.753079	58.848705
2411.108869	111470.469321	58.853709
2410.344579	111309.919246	58.858714
2409.814052	111147.105683	58.863719
2409.099713	111022.772942	58.868724
2408.596250	110865.217813	58.873729
2408.050267	110700.207588	58.878733
2406.866671	110588.072213	58.883738
2406.003853	110403.086482	58.888743
2405.717875	110292.936012	58.893748
2404.804068	110126.464951	58.898753
2404.195065	109992.589319	58.903757
2403.422143	109852.064693	58.908762
2402.855931	109692.743879	58.913767
2402.642322	109566.086403	58.918772
2401.777063	109410.476285	58.923777
2401.366871	109246.659978	58.928781
2400.918553	109126.863487	58.933786
2400.011984	108945.734762	58.938791
2399.210068	108827.309324	58.943796
2398.368635	108655.011674	58.948801
2398.020712	108512.498373	58.953805
2396.922250	108382.148379	58.958810
2396.421270	108209.044818	58.963815
2395.678162	108092.802770	58.968820
2394.882920	107929.310195	58.973825
2394.419067	107789.966756	58.978829
2393.385107	107656.310941	58.983834
2393.295589	107494.168804	58.988839
2392.393942	107348.799660	58.993844
2391.736001	107209.179434	58.998849
2391.195376	107064.306786	59.003853
2390.400955	106917.743071	59.008858
2389.879103	106770.686544	59.013863
2389.082512	106628.674251	59.018868
2388.643632	106481.530199	59.023873
2387.868728	106328.545995	59.028877
2387.504067	106190.198564	59.033882
2386.522517	106034.723778	59.038887
2385.980084	105895.130947	59.043892
2385.195232	105743.497134	59.048897
2384.860127	105591.006244	59.053901
2384.092158	105453.177490	59.058906
2383.240247	105305.052960	59.063911
2382.762530	105153.672393	59.068916
2382.148840	105015.834397	59.073921
2381.547724	104855.199688	59.078925
2380.455725	104713.416921	59.083930
2380.089954	104551.795292	59.088935
2379.392329	104404.920777	59.093940
2378.587744	104259.510623	59.098945
2377.996383	104107.247516	59.103949
2377.091721	103967.253960	59.108954
2376.476133	103825.464415	59.113959
2375.951024	103663.449056	59.118964
2375.344384	103512.486401	59.123969
2374.438418	103390.748345	59.128973
2373.927374	103233.682052	59.133978
2373.116154	103085.260448	59.138983
2372.665759	102948.791589	59.143988
2371.651919	102802.440294	59.148993
2371.624761	102659.593857	59.153997
2370.663192	102519.040649	59.159002
2369.776301	102369.081343	59.164007
2369.559790	102221.319472	59.169012
2368.638884	102077.920482	59.174017
2367.957450	101919.120122	59.179021
2367.397086	101772.468650	59.184026
2366.596132	101624.809562	59.189031
2366.054631	101490.203282	59.194036
2365.292202	101333.551172	59.199041
2364.850416	101185.964786	59.204045
2364.055172	101049.675874	59.209050
2363.501277	100880.757343	59.214055
2363.195917	100745.794418	59.219060
2362.183431	100610.639923	59.224065
2361.904582	100441.763440	59.229069
2360.642885	100291.826201	59.234074
2360.479501	100139.831869	59.239079
2359.373164	99996.329237	59.244084
2358.634345	99840.837917	59.249089
2358.338808	99684.141956	59.254093
2357.440303	99546.926816	59.259098
2356.812203	99398.645581	59.264103
2356.510327	99249.064023	59.269108
2355.584960	99100.711329	59.274113
2355.102793	98943.142975	59.279117
2354.067001	98799.046743	59.284122
2353.294313	98655.563000	59.289127
2352.703082	98517.683699	59.294132
2352.182905	98360.245889	59.299137
2351.879434	98211.229503	59.304141
2350.609172	98065.684554	59.309146
2350.281356	97912.950883	59.314151
2349.869216	97774.273880	59.319156
2349.082464	97625.902427	59.324161
2348.304218	97454.031975	59.329165
2347.610334	97339.903010	59.334170
2347.106500	97171.485826	59.339175
2346.666662	97018.566618	59.344180
2345.419086	96868.097781	59.349185
2345.243022	96719.121691	59.354189
2344.824910	96567.032909	59.359194
2343.784203	96409.906761	59.364199
2343.376921	96256.410400	59.369204
2342.583814	96105.868224	59.374209
2341.876468	95951.590709	59.379213
2341.078786	95807.995720	59.384218
2339.978348	95650.212086	59.389223
2339.469336	95505.939058	59.394228
2338.861728	95353.628481	59.399233
2338.461535	95200.043059	59.404237
2337.838439	95054.966583	59.409242
2336.981532	94899.946303	59.414247
2336.211603	94774.325865	59.419252
2335.930920	94608.974457	59.424257
2335.402641	94450.195338	59.429261
2334.370335	94303.584202	59.434266
2333.701453	94162.947144	59.439271
2333.367730	93998.635977	59.444276
2332.474414	93853.229655	59.449281
2332.325100	93700.623015	59.454285
2331.285587	93560.600225	59.459290
2330.758246	93387.941054	59.464295
2330.270887	93239.665187	59.469300
2329.260869	93104.954530	59.474305
2329.085031	92933.200669	59.479309
2328.002947	92779.017139	59.484314
2327.062341	92629.117814	59.489319
2326.596805	92462.169323	59.494324
2325.798713	92332.477189	59.499329
2325.511391	92168.489243	59.504333
2324.870093	92021.120987	59.509338
2324.090760	91859.901882	59.514343
2323.484698	91704.756306	59.519348
2322.693882	91550.332260	59.524353
2322.259951	91392.993053	59.529357
2321.422741	91243.289650	59.534362
2320.617053	91087.685511	59.539367
2320.100186	90929.221468	59.544372
2319.274999	90768.195174	59.549377
2318.615168	90627.724984	59.554381
2318.118021	90483.121302	59.559386
2317.417966	90327.404363	59.564391
2316.613011	90168.858358	59.569396
2315.893875	90015.207277	59.574401
2315.940501	89861.835279	59.579405
2315.042144	89719.278432	59.584410
2314.056850	89559.801741	59.589415
2313.542674	89387.317687	59.594420
2312.724520	89241.942582	59.599425
2312.185863	89092.193892	59.604429
2311.270099	88928.589794	59.609434
2310.379187	88783.552635	59.614439
2310.227495	88612.754389	59.619444
2309.305257	88490.211729	59.624449
2309.077848	88320.467529	59.629453
2308.063184	88158.102175	59.634458
2307.232702	88025.220155	59.639463
2307.062467	87846.303395	59.644468
2306.040061	87703.189894	59.649473
2305.731463	87555.919500	59.654477
2304.957071	87406.156471	59.659482
2304.397430	87243.294761	59.664487
2303.799689	87097.569473	59.669492
2302.502096	86921.780675	59.674497
2302.730818	86781.676285	59.679501
2301.784832	86627.755592	59.684506
2300.851215	86458.854400	59.689511
2300.399779	86318.188942	59.694516
2299.532267	86154.065773	59.699521
2299.023016	85993.589087	59.704525
2298.375797	85841.686881	59.709530
2297.483383	85696.582038	59.714535
2296.954801	85534.184810	59.719540
2296.356551	85381.175139	59.724545
2296.023304	85219.465631	59.729549
2295.041970	85064.230657	59.734554
2294.453990	84909.416185	59.739559
2293.850115	84751.835332	59.744564
2292.678812	84595.321798	59.749569
2292.609282	84439.978482	59.754573
2291.902913	84284.084425	59.759578
2291.116452	84122.778419	59.764583
2290.522982	83959.452747	59.769588
2289.746556	83804.188174	59.774593
2289.045055	83651.562317	59.779597
2288.558428	83501.223328	59.784602
2287.803639	83336.926598	59.789607
2287.042231	83192.033640	59.794612
2286.014096	83051.627079	59.799617
2285.687881	82871.198612	59.804621
2284.887148	82738.452627	59.809626
2284.311056	82580.072306	59.814631
2283.887501	82419.127435	59.819636
2282.814884	82278.720428	59.824641
2282.644926	82121.324932	59.829645
2281.822489	81961.549643	59.834650
2281.266953	81800.148783	59.839655
2280.811162	81627.496431	59.844660
2279.938076	81477.670548	59.849665
2279.226586	81317.793862	59.854669
2278.512193	81167.945039	59.859674
2277.893978	81006.002553	59.864679
2277.352628	80846.241933	59.869684
2276.239115	80690.464519	59.874689
2276.148641	80525.678922	59.879693
2275.289066	80369.172862	59.884698
2274.261459	80225.629206	59.889703
2273.520456	80070.564194	59.894708
2273.175002	79918.105603	59.899713
2272.720488	79746.070725	59.904718
2271.762033	79610.175744	59.909722
2271.220550	79433.182576	59.914727
2270.868677	79272.979457	59.919732
2270.065250	79128.241852	59.924737
2269.158240	78978.743603	59.929742
2268.635122	78812.031458	59.934746
2267.982680	78663.325266	59.939751
2267.744534	78483.795414	59.944756
2266.352291	78355.258549	59.949761
2266.180818	78176.487564	59.954766
2265.259146	78021.156140	59.959770
2264.825031	77866.344211	59.964775
2264.253442	77706.302219	59.969780
2263.090876	77548.870819	59.974785
2262.551583	77387.983437	59.979790
2261.656355	77240.080133	59.984794
2261.164006	77082.995919	59.989799
2260.923395	76919.093090	59.994804
2259.988358	76768.468557	59.999809
2259.711044	76598.998179	60.004814
2258.819132	76442.983404	60.009818
2258.116776	76285.710549	60.014823
2257.367017	76129.719990	60.019828
2256.795125	75971.446784	60.024833
2256.199215	75807.115065	60.029838
2255.399421	75653.911276	60.034842
2254.734707	75502.068452	60.039847
2254.245289	75347.461872	60.044852
2253.400314	75192.190588	60.049857
2253.012867	75026.679033	60.054862
2252.017822	74867.189095	60.059866
2251.242293	74707.855673	60.064871
2250.989652	74547.864037	60.069876
2250.197086	74401.244982	60.074881
2249.488760	74245.610868	60.079886
2248.554431	74091.559661	60.084890
2247.763120	73931.829426	60.089895
2247.425287	73771.084568	60.094900
2246.831799	73606.909797	60.099905
2246.140043	73447.427382	60.104910
2245.526393	73310.689945	60.109914
2244.389642	73136.905981	60.114919
2244.353601	72982.112660	60.119924
2243.155133	72835.062648	60.124929
2242.692755	72667.035754	60.129934
2242.165608	72522.238197	60.134938
2241.462951	72366.833199	60.139943
2240.771651	72206.087319	60.144948
2239.510428	72054.301883	60.149953
2239.367539	71895.986451	60.154958
2238.819356	71745.008824	60.159962
2237.944791	71591.676940	60.164967
2237.758659	71433.967512	60.169972
2236.599128	71282.957348	60.174977
2236.154416	71125.038012	60.179982
2235.464334	70965.619581	60.184986
2234.848843	70814.285996	60.189991
2234.334704	70656.704472	60.194996
2233.384526	70506.883238	60.200001
2232.933145	70335.371487	60.205006
2232.283792	70182.933288	60.210010
2231.145214	70026.475662	60.215015
2231.154712	69868.868057	60.220020
2230.101821	69718.670071	60.225025
2229.706043	69558.430926	60.230030
2229.213925	69401.229674	60.235034
2228.367377	69236.770227	60.240039
2228.056498	69085.224285	60.245044
2227.068528	68929.080889	60.250049
2226.481098	68755.900724	60.255054
2225.808439	68595.143342	60.260058
2225.289964	68448.569223	60.265063
2224.781116	68283.044518	60.270068
2223.814385	68122.850697	60.275073
2223.150404	67958.955742	60.280078
2222.374779	67797.581588	60.285082
2221.930766	67634.952828	60.290087
2221.179880	67472.931440	60.295092
2220.500126	67323.598373	60.300097
2219.893801	67156.635726	60.305102
2219.422924	66989.165377	60.310106
2218.500093	66834.301436	60.315111
2218.164204	66666.400812	60.320116
2217.307113	66501.193527	60.325121
2216.538682	66330.229587	60.330126
2215.851117	66185.285793	60.335130
2215.251315	66014.722207	60.340135
2214.663329	65849.974941	60.345140
2213.972638	65705.418388	60.350145
2213.584231	65533.486150	60.355150
2212.663882	65371.189468	60.360154
2211.793476	65203.753664	60.365159
2211.456453	65031.368153	60.370164
2210.850736	64884.157297	60.375169
2209.927590	64723.636470	60.380174
2209.116054	64570.007921	60.385178
2208.602638	64395.300463	60.390183
2208.181714	64225.864212	60.395188
2207.009366	64089.112130	60.400193
2206.668715	63917.256469	60.405198
2205.699206	63745.283652	60.410202
2205.063297	63610.169081	60.415207
2204.919478	63439.014695	60.420212
2204.280823	63259.392200	60.425217
2203.427737	63123.226440	60.430222
2203.037003	62948.645745	60.435226
2202.291624	62784.719172	60.440231
2201.415854	62619.918758	60.445236
2200.523281	62457.499992	60.450241
2199.808241	62280.703814	60.455246
2199.440809	62140.105584	60.460250
2198.540691	61979.781537	60.465255
2198.054222	61806.135129	60.470260
2197.094725	61654.051014	60.475265
2196.738702	61488.693657	60.480270
2195.701046	61332.119773	60.485274
2195.400322	61174.711691	60.490279
2194.703579	61006.436923	60.495284
2193.687570	60859.524954	60.500289
2193.391461	60710.109942	60.505294
2192.920744	60535.098903	60.510298
2192.409297	60367.515870	60.515303
2191.832706	60206.291427	60.520308
2190.462982	60056.232078	60.525313
2190.081753	59887.920452	60.530318
2189.458634	59721.085797	60.535322
2188.725163	59561.721385	60.540327
2188.288687	59400.380367	60.545332
2187.180002	59256.078591	60.550337
2186.633939	59076.095130	60.555342
2186.219627	58922.990771	60.560346
2185.523784	58750.323786	60.565351
2184.825890	58594.497548	60.570356
2184.155233	58429.856474	60.575361
2183.543239	58270.553469	60.580366
2182.873529	58113.223356	60.585370
2182.021513	57945.111573	60.590375
2181.792992	57783.194533	60.595380
2180.781473	57622.792567	60.600385
2180.118434	57457.877225	60.605390
2179.461574	57293.589038	60.610394
2178.827997	57142.072332	60.615399
2178.205028	56981.975091	60.620404
2177.123934	56822.844416	60.625409
2176.795363	56652.816214	60.630414
2176.122726	56490.003014	60.635418
2175.228731	56326.928879	60.640423
2174.965822	56183.450493	60.645428
2174.189187	56021.629524	60.650433
2173.577745	55849.099665	60.655438
2173.075962	55688.858364	60.660442
2172.248853	55526.796589	60.665447
2171.743797	55360.292637	60.670452
2171.041886	55219.423140	60.675457
2170.467293	55044.743068	60.680462
2169.742056	54885.575897	60.685466
2169.125655	54720.598594	60.690471
2168.508431	54546.892060	60.695476
2167.376542	54390.625944	60.700481
2166.704419	54233.987606	60.705486
2166.135138	54071.882011	60.710490
2165.560586	53905.914978	60.715495
2165.224930	53739.822957	60.720500
2164.110185	53590.070082	60.725505
2163.766951	53419.871720	60.730510
2163.209953	53257.894841	60.735514
2162.518595	53102.367309	60.740519
2161.994617	52919.067535	60.745524
2161.285055	52772.418184	60.750529
2160.509750	52601.245543	60.755534
2159.887194	52438.814931	60.760538
2159.013447	52280.817404	60.765543
2158.358007	52118.942275	60.770548
2157.638528	51952.421282	60.775553
2157.080794	51777.263716	60.780558
2156.298417	51623.712386	60.785562
2155.588513	51465.161302	60.790567
2155.154810	51295.471889	60.795572
2154.494345	51134.384734	60.800577
2153.743146	50979.783542	60.805582
2152.834932	50813.575129	60.810586
2152.191310	50632.605048	60.815591
2152.030673	50499.573783	60.820596
2151.304589	50330.648569	60.825601
2150.809649	50163.947182	60.830606
2150.074096	49988.174064	60.835610
2149.453354	49828.079428	60.840615
2149.057931	49657.194096	60.845620
2148.073333	49495.125953	60.850625
2147.367183	49330.968268	60.855630
2146.735249	49164.152428	60.860634
2145.973653	49002.306474	60.865639
2145.346447	48821.478686	60.870644
2144.348840	48665.446619	60.875649
2144.040427	48490.003297	60.880654
2143.358135	48341.509967	60.885658
2142.722125	48179.034727	60.890663
2142.343543	47997.021260	60.895668
2141.472384	47834.690877	60.900673
2140.819097	47669.094537	60.905678
2140.451268	47505.728841	60.910682
2139.220377	47333.983012	60.915687
2138.909693	47154.523331	60.920692
2137.959718	46995.018925	60.925697
2137.504669	46827.229098	60.930702
2136.866830	46666.330649	60.935706
2136.028934	46501.068734	60.940711
2135.354748	46321.659393	60.945716
2134.607167	46167.390525	60.950721
2133.889209	45991.945269	60.955726
2133.824366	45835.448631	60.960730
2133.068048	45681.960341	60.965735
2132.415666	45494.490527	60.970740
2131.511154	45337.287065	60.975745
2130.967217	45158.903213	60.980750
2130.498060	44989.463216	60.985754
2129.463888	44824.172349	60.990759
2129.093710	44656.949630	60.995764
2128.208082	44491.755366	61.000769
2127.624287	44310.176355	61.005774
2126.764683	44149.225531	61.010778
2126.174686	43983.916439	61.015783
2125.572617	43814.452024	61.020788
2124.774773	43659.109540	61.025793
2124.101952	43491.462164	61.030798
2123.396802	43324.782937	61.035802
2122.671465	43161.258340	61.040807
2122.083575	42987.802383	61.045812
2121.254245	42827.820394	61.050817
2120.665496	42663.162498	61.055822
2120.109861	42510.075129	61.060826
2119.098982	42338.947552	61.065831
2118.946070	42168.744911	61.070836
2118.377887	42010.363963	61.075841
2117.791526	41837.747822	61.080846
2117.126654	41663.735526	61.085850
2116.404581	41511.543547	61.090855
2115.869710	41337.007982	61.095860
2114.796069	41161.260048	61.100865
2114.418144	40992.764837	61.105870
2113.756639	40844.240330	61.110874
2112.859223	40673.399067	61.115879
2112.311830	40501.650234	61.120884
2111.184219	40336.638453	61.125889
2110.617569	40164.774320	61.130894
2109.993603	40021.763806	61.135898
2109.301579	39854.045805	61.140903
2109.039065	39685.317492	61.145908
2108.317746	39532.689253	61.150913
2107.869892	39360.439691	61.155918
2107.267231	39190.786930	61.160922
2106.203690	39021.061969	61.165927
2105.743204	38851.753625	61.170932
2104.906229	38697.307968	61.175937
2104.332870	38530.048938	61.180942
2103.864305	38356.160885	61.185946
2102.782942	38191.040835	61.190951
2102.309112	38028.881610	61.195956
2101.598031	37862.055696	61.200961
2101.046929	37692.276946	61.205966
2100.593287	37531.342769	61.210970
2099.574824	37370.107733	61.215975
2099.477977	37194.832190	61.220980
2098.651700	37026.744540	61.225985
2097.816333	36863.708618	61.230990
2097.110322	36695.481898	61.235994
2096.509097	36516.888735	61.240999
2096.131357	36346.977465	61.246004
2095.082636	36178.029478	61.251009
2094.511119	36004.945395	61.256014
2093.964144	35848.301749	61.261018
2093.185311	35688.198611	61.266023
2092.698110	35509.582258	61.271028
2091.448391	35343.462622	61.276033
2090.876004	35172.972982	61.281038
2090.264746	35014.624590	61.286042
2089.747864	34852.321041	61.291047
2089.165767	34684.714366	61.296052
2088.628587	34525.118205	61.301057
2087.613978	34358.209292	61.306062
2087.065660	34194.927782	61.311066
2086.372301	34025.094896	61.316071
2085.787521	33850.360009	61.321076
2084.988226	33708.255819	61.326081
2084.502882	33535.615075	61.331086
2083.621865	33358.993282	61.336090
2082.866882	33204.013066	61.341095
2082.554170	33028.548313	61.346100
2081.508508	32876.978561	61.351105
2081.146405	32717.752812	61.356110
2080.598791	32559.691069	61.361114
2079.440275	32378.400405	61.366119
2079.093174	32220.769929	61.371124
2078.429141	32073.288729	61.376129
2077.665141	31891.503090	61.381134
2076.882843	31731.839957	61.386138
2076.092093	31581.873952	61.391143
2075.545468	31403.652468	61.396148
2074.869565	31256.110937	61.401153
2074.491469	31090.609792	61.406158
2073.951531	30927.826889	61.411162
2072.887680	30757.184119	61.416167
2072.323467	30609.377858	61.421172
2071.549900	30447.763371	61.426177
2070.865816	30277.123794	61.431182
2070.238409	30121.602461	61.436186
2069.673910	29962.405446	61.441191
2069.192701	29799.818760	61.446196
2068.270739	29659.243064	61.451201
2067.884810	29486.948104	61.456206
2067.326907	29318.401420	61.461210
2066.399446	29152.518828	61.466215
2065.844582	28995.585831	61.471220
2065.146110	28842.438851	61.476225
2064.375567	28670.711212	61.481230
2063.810505	28507.428708	61.486234
2062.828033	28365.101180	61.491239
2062.283396	28171.507962	61.496244
2061.390365	28035.801231	61.501249
2060.868188	27878.003353	61.506254
2060.197767	27718.554389	61.511258
2059.334797	27572.232226	61.516263
2058.875766	27414.139746	61.521268
2057.898443	27241.011417	61.526273
2057.497346	27097.996138	61.531278
2056.779637	26944.782448	61.536282
2056.294955	26789.420396	61.541287
2055.687176	26632.337782	61.546292
2054.666112	26482.520791	61.551297
2054.125252	26324.410096	61.556302
2053.474544	26178.787979	61.561306
2052.818202	26016.775619	61.566311
2052.611234	25853.900617	61.571316
2051.842243	25708.005356	61.576321
2050.844000	25543.607613	61.581326
2050.486325	25385.951728	61.586330
2049.580921	25231.739250	61.591335
2049.277692	25069.504283	61.596340
2048.149909	24925.656952	61.601345
2047.453952	24762.639221	61.606350
2046.734160	24608.317994	61.611354
2045.749987	24463.182133	61.616359
2045.199543	24315.299227	61.621364
2044.275903	24170.082977	61.626369
2043.501138	24029.284958	61.631374
2042.905730	23888.469193	61.636378
2042.246027	23727.909080	61.641383
2041.507921	23607.621288	61.646388
2040.692712	23480.141581	61.651393
2039.854790	23329.746968	61.656398
2039.318965	23196.529273	61.661402
2038.447530	23075.739953	61.666407
2037.727324	22932.729548	61.671412
2036.715132	22811.466305	61.676417
2036.098349	22700.600850	61.681422
2035.085290	22556.991220	61.686426
2034.065080	22441.055812	61.691431
2033.670261	22338.523799	61.696436
2032.866490	22215.608569	61.701441
2032.000606	22088.972440	61.706446
2031.501862	22008.062884	61.711450
2030.529860	21889.548951	61.716455
2029.891863	21763.513312	61.721460
2029.030391	21673.224991	61.726465
2028.410941	21561.476487	61.731470
2027.694678	21458.701148	61.736474
2026.870103	21359.889182	61.741479
2026.455807	21253.882102	61.746484
2025.431390	21169.356393	61.751489
2024.622898	21065.517337	61.756494
2024.008909	20969.209683	61.761498
2023.652425	20878.441515	61.766503
2022.731201	20772.196781	61.771508
2021.997628	20700.684966	61.776513
2021.077955	20605.193912	61.781518
2020.606732	20496.986699	61.786522
2019.628015	20414.950351	61.791527
2019.245635	20329.791564	61.796532
2018.373986	20247.557507	61.801537
2017.926000	20165.848385	61.806542
2017.486346	20072.763467	61.811546
2016.874735	19979.140710	61.816551
2015.835762	19888.126959	61.821556
2014.820782	19824.328296	61.826561
2014.774238	19724.467178	61.831566
2014.050493	19636.890870	61.836570
2013.205031	19549.305159	61.841575
2012.705912	19467.214629	61.846580
2011.904276	19384.272144	61.851585
2010.986934	19299.070044	61.856590
2010.389519	19221.372850	61.861594
2009.895896	19135.956759	61.866599
2009.399952	19054.683802	61.871604
2008.523765	18970.706941	61.876609
2007.682781	18877.017844	61.881614
2007.512709	18794.233642	61.886618
2006.672235	18720.966054	61.891623
2006.461668	18629.757102	61.896628
2005.293379	18560.353712	61.901633
2004.938425	18467.356477	61.906638
2004.307683	18388.486940	61.911642
2003.423773	18288.854333	61.916647
2003.053833	18204.864797	61.921652
2002.120812	18129.190381	61.926657
2001.475463	18032.600265	61.931662
2000.724886	17953.399482	61.936666
1999.936777	17887.462266	61.941671
1999.737438	17787.984320	61.946676
1998.838327	17708.941372	61.951681
1998.259755	17625.835094	61.956686
1997.766062	17541.848650	61.961690
1996.854682	17462.725623	61.966695
1996.467949	17366.209904	61.971700
1995.686127	17293.279168	61.976705
1994.764881	17208.568873	61.981710
1994.272409	17120.885145	61.986714
1993.663524	17040.754817	61.991719
1993.284152	16954.284690	61.996724
1992.765290	16869.839766	62.001729
1991.688254	16786.963129	62.006734
1990.934286	16698.662811	62.011738
1990.392489	16631.539603	62.016743
1989.802732	16539.277111	62.021748
1988.995108	16460.027104	62.026753
1988.398833	16370.798662	62.031758
1987.999255	16295.034526	62.036762
1987.130138	16206.807587	62.041767
1986.603673	16116.478106	62.046772
1986.156374	16033.289883	62.051777
1985.532562	15945.313402	62.056782
1984.769572	15861.397565	62.061786
1983.879781	15774.625728	62.066791
1983.218623	15685.318214	62.071796
1982.597578	15614.352777	62.076801
1981.833062	15521.563910	62.081806
1981.402839	15442.430504	62.086810
1980.848902	15358.257013	62.091815
1980.028597	15267.162350	62.096820
1979.136801	15188.465688	62.101825
1978.491898	15095.124596	62.106830
1978.281982	15016.099000	62.111834
1977.130942	14919.086701	62.116839
1976.627887	14838.206949	62.121844
1975.977935	14771.225129	62.126849
1975.380733	14672.909958	62.131854
1974.783525	14591.428576	62.136858
1973.989788	14516.824794	62.141863
1973.355731	14431.386600	62.146868
1972.493423	14345.456235	62.151873
1971.992675	14261.732558	62.156878
1971.046582	14182.546946	62.161882
1970.447917	14103.304426	62.166887
1970.286313	14022.735246	62.171892
1969.458632	13933.579966	62.176897
1968.781748	13855.139262	62.181902
1967.929671	13769.950672	62.186906
1967.260551	13687.233955	62.191911
1967.009004	13602.804775	62.196916
1966.203824	13524.437429	62.201921
1965.496915	13439.195949	62.206926
1964.830660	13344.060717	62.211930
1964.030500	13271.189156	62.216935
1963.648961	13178.185591	62.221940
1962.723867	13099.044187	62.226945
1962.016807	13023.404186	62.231950
1961.603272	12922.211517	62.236954
1960.786205	12853.811310	62.241959
1959.973807	12775.853788	62.246964
1959.386024	12699.514645	62.251969
1958.732125	12617.474643	62.256974
1958.295272	12532.322048	62.261978
1957.361580	12456.924825	62.266983
1956.724054	12369.401326	62.271988
1955.926648	12288.699563	62.276993
1955.190361	12210.691034	62.281998
1955.109159	12118.576032	62.287002
1954.278896	12052.796621	62.292007
1953.522008	11950.586408	62.297012
1953.117230	11882.882856	62.302017
1952.361125	11796.937176	62.307022
1951.388508	11713.945964	62.312026
1950.675219	11647.220006	62.317031
1950.039621	11552.469178	62.322036
1948.976689	11479.919853	62.327041
1948.600643	11393.617072	62.332046
1948.248283	11316.269659	62.337050
1947.496574	11241.769443	62.342055
1946.631054	11166.583821	62.347060
1946.046009	11091.176909	62.352065
1945.264479	11005.207012	62.357070
1944.861300	10923.913779	62.362074
1944.164931	10865.238015	62.367079
1943.487224	10777.046777	62.372084
1942.772914	10687.026972	62.377089
1941.972047	10614.818345	62.382094
1941.767423	10543.454946	62.387098
1940.777331	10470.250924	62.392103
1940.021722	10384.292282	62.397108
1939.717706	10296.009422	62.402113
1938.915834	10237.186368	62.407118
1938.162512	10156.496473	62.412122
1937.210170	10089.035810	62.417127
1936.844648	10001.791319	62.422132
1936.200634	9939.207294	62.427137
1935.305371	9856.275555	62.432142
1934.784232	9778.153308	62.437146
1933.757959	9710.035839	62.442151
1933.100989	9631.612433	62.447156
1932.291023	9566.434141	62.452161
1931.616217	9498.855144	62.457166
1931.012644	9423.609417	62.462170
1930.711771	9361.736647	62.467175
1929.818738	9287.316653	62.472180
1929.044989	9212.130558	62.477185
1928.542901	9153.132009	62.482190
1927.805788	9077.244919	62.487194
1926.908886	9026.776525	62.492199
1926.689557	8955.319436	62.497204
1925.686473	8884.545278	62.502209
1925.040503	8809.445057	62.507214
1924.258085	8751.173835	62.512218
1923.216185	8683.823250	62.517223
1922.928473	8614.493357	62.522228
1922.152164	8561.307697	62.527233
1921.206672	8489.875010	62.532238
1920.842509	8434.273009	62.537242
1920.174451	8374.620674	62.542247
1919.435759	8309.296111	62.547252
1918.633890	8247.548100	62.552257
1918.309398	8194.737749	62.557262
1917.712281	8119.769714	62.562266
1916.726065	8069.619302	62.567271
1916.194508	8011.762781	62.572276
1915.663312	7954.606170	62.577281
1914.835728	7892.009347	62.582286
1914.141166	7830.846366	62.587290
1913.475106	7772.579029	62.592295
1912.998250	7710.313050	62.597300
1912.427992	7649.478185	62.602305
1911.734924	7587.940460	62.607310
1911.095986	7509.144284	62.612314
1910.315423	7454.419438	62.617319
1909.900200	7396.537368	62.622324
1909.322164	7336.302181	62.627329
1908.362805	7271.705864	62.632334
1907.878003	7202.830321	62.637338
1906.892634	7141.549101	62.642343
1906.102504	7087.661721	62.647348
1905.468018	7026.444387	62.652353
1904.621881	6972.758791	62.657358
1904.367329	6908.667058	62.662362
1903.549299	6850.381703	62.667367
1903.049732	6802.662841	62.672372
1902.181331	6735.418550	62.677377
1901.490605	6676.642740	62.682382
1900.954997	6623.776810	62.687386
1900.041788	6574.017420	62.692391
1899.842639	6496.968692	62.697396
1899.275265	6444.307226	62.702401
1898.043172	6384.664849	62.707406
1897.747271	6324.725790	62.712410
1896.972633	6269.239232	62.717415
1896.180839	6206.759776	62.722420
1895.478416	6158.907965	62.727425
1894.620488	6111.981007	62.732430
1894.400321	6043.759803	62.737434
1893.785302	5996.712612	62.742439
1893.024295	5931.816537	62.747444
1892.180687	5880.646764	62.752449
1891.692369	5827.779320	62.757454
1891.256328	5756.091549	62.762458
1890.510316	5710.205052	62.767463
1890.074157	5641.815698	62.772468
1889.392206	5585.405964	62.777473
1888.590554	5520.503948	62.782478
1888.010355	5462.452109	62.787482
1887.081694	5406.363813	62.792487
1886.606600	5338.469491	62.797492
1885.897955	5288.920940	62.802497
1884.954874	5236.030007	62.807502
1884.575758	5179.593463	62.812506
1883.465609	5121.520621	62.817511
1883.066910	5061.148682	62.822516
1882.482353	4997.287967	62.827521
1881.838931	4947.923445	62.832526
1880.989383	4886.569269	62.837530
1880.234063	4844.294573	62.842535
1879.674835	4778.800492	62.847540
1878.935877	4731.665799	62.852545
1878.464237	4687.219346	62.857550
1878.076776	4622.917251	62.862554
1877.141301	4569.791678	62.867559
1876.636472	4507.795185	62.872564
1875.925545	4453.073536	62.877569
1875.256423	4405.973754	62.882574
1874.719235	4339.486731	62.887578
1873.702610	4290.468386	62.892583
1873.494681	4228.041838	62.897588
1872.802108	4166.076591	62.902593
1871.719631	4113.534398	62.907598
1871.333117	4047.830016	62.912602
1870.561219	4003.372571	62.917607
1869.806197	3933.975464	62.922612
1868.849734	3883.486725	62.927617
1868.814451	3829.616784	62.932622
1868.182230	3777.701490	62.937626
1867.305611	3724.513636	62.942631
1867.001637	3668.208966	62.947636
1866.241440	3601.083229	62.952641
1865.334824	3540.461409	62.957646
1864.976010	3491.944612	62.962650
1863.972376	3439.540584	62.967655
1863.161135	3375.095137	62.972660
1862.829310	3323.662147	62.977665
1861.877055	3276.212681	62.982670
1861.258035	3218.040211	62.987674
1860.450146	3167.214109	62.992679
1860.085026	3097.777190	62.997684
1859.387949	3047.726481	63.002689
1858.722748	2997.306538	63.007694
1858.292244	2935.458661	63.012698
1857.281831	2883.445704	63.017703
1856.585096	2823.564798	63.022708
1856.083900	2768.637906	63.027713
1855.097127	2718.174562	63.032718
1854.884857	2665.489149	63.037722
1854.047559	2617.584316	63.042727
1853.257287	2562.537702	63.047732
1852.573294	2508.277212	63.052737
1851.900599	2456.196385	63.057742
1851.451673	2407.360758	63.062746
1850.659175	2356.333153	63.067751
1849.995288	2296.524108	63.072756
1849.137759	2243.225844	63.077761
1848.249786	2197.479329	63.082766
1848.061125	2134.557089	63.087770
1847.165757	2097.536888	63.092775
1846.467719	2043.448325	63.097780
1845.994452	1984.226169	63.102785
1845.058178	1944.487557	63.107790
1844.736376	1887.277826	63.112794
1843.914470	1831.086115	63.117799
1843.357153	1783.480228	63.122804
1842.496265	1731.605353	63.127809
1842.131780	1694.271627	63.132814
1841.620404	1631.830980	63.137818
1840.557957	1597.870559	63.142823
1840.197490	1535.789597	63.147828
1839.362979	1489.405983	63.152833
1838.861546	1429.342082	63.157838
1837.841557	1377.755528	63.162842
1837.138245	1347.291030	63.167847
1836.471123	1289.378330	63.172852
1835.848802	1236.394939	63.177857
1835.266782	1181.468721	63.182862
1835.031909	1134.461139	63.187866
1833.892005	1098.467970	63.192871
1833.077238	1037.165420	63.197876
1832.734514	983.080365	63.202881
1831.834384	950.946336	63.207886
1831.333914	906.268355	63.212890
1830.424923	858.950793	63.217895
1829.758130	805.570742	63.222900
1829.475714	766.524771	63.227905
1828.713137	715.790709	63.232910
1828.312688	660.828956	63.237914
1826.954470	619.082496	63.242919
1826.181123	570.375511	63.247924
1825.945464	525.208791	63.252929
1825.115000	489.633214	63.257934
1824.342621	436.365908	63.262938
1823.678803	400.303614	63.267943
1823.242632	346.604779	63.272948
1822.490159	316.703771	63.277953
1821.599633	285.676722	63.282958
1820.974672	223.737193	63.287962
1820.342000	205.217159	63.292967
1819.734543	168.406907	63.297972
1818.912311	116.061746	63.302977
1818.050329	76.043656	63.307982
1817.815143	38.272617	63.312986
1816.342093	14.510525	63.317991
1815.642379	-32.430502	63.322996
1815.105841	-46.628944	63.328001
1814.046272	-72.184852	63.333006
1812.530891	-73.432728	63.338010
1808.659990	-1.503316	63.343015
1808.276339	-12.763026	63.348020
1809.105462	-5.101430	63.353025
1808.935162	3.177758	63.358030
1808.567597	-2.593662	63.363034
1808.259132	5.366851	63.368039
1807.843914	-7.209313	63.373044
1806.814437	1.356115	63.378049
1806.448242	-2.125828	63.383054
1805.431945	7.637549	63.388058
1804.258354	9.377284	63.393063
1804.009277	6.378203	63.398068
1803.768575	15.575309	63.403073
1803.344949	13.269408	63.408078
1802.784547	12.905922	63.413082
1801.763880	28.708057	63.418087
1801.180867	23.420265	63.423092
1800.046838	19.393208	63.428097
1799.323184	18.183607	63.433102
1798.664103	12.455321	63.438106
1797.788998	21.753173	63.443111
1797.458134	20.761890	63.448116
1797.457982	18.852359	63.453121
1796.965252	27.343608	63.458126
1795.890876	7.634015	63.463130
1794.787206	16.771045	63.468135
1794.237054	23.945217	63.473140
1793.699608	28.043943	63.478145
1792.902412	29.449527	63.483150
1792.615850	17.959918	63.488154
1791.719078	25.307404	63.493159
1791.147068	27.049383	63.498164
1790.490513	20.663117	63.503169
1789.616156	25.170154	63.508174
1789.203959	20.541204	63.513178
1789.103698	30.972827	63.518183
1788.245099	24.058836	63.523188
1787.673653	23.723915	63.528193
1786.428361	22.357461	63.533198
1786.250099	27.187612	63.538202
1785.202433	25.606852	63.543207
1784.448211	24.797917	63.548212
1783.792125	21.480277	63.553217
1783.342845	30.144399	63.558222
1783.219858	15.921234	63.563226
1782.091536	25.860113	63.568231
1781.373834	20.126946	63.573236
1780.692251	24.983411	63.578241
1779.742207	24.834769	63.583246
1779.507243	13.581396	63.588250
1778.369338	24.400144	63.593255
1778.418110	30.466821	63.598260
1778.196678	22.350955	63.603265
1777.086521	19.132235	63.608270
1776.109597	21.805829	63.613274
1775.512528	21.181671	63.618279
1774.822667	26.807415	63.623284
1774.379960	17.469882	63.628289
1773.692495	28.180831	63.633294
1773.598948	19.746619	63.638298
1772.473854	25.531366	63.643303
1771.536683	28.974498	63.648308
1770.776774	20.100493	63.653313
1770.160981	23.002162	63.658318
1769.723709	16.024426	63.663322
1768.669743	21.685915	63.668327
1768.349647	15.058572	63.673332
1767.681847	20.895274	63.678337
1766.560548	18.514099	63.683342
1766.556685	20.361394	63.688346
1765.385570	18.218362	63.693351
1764.833121	26.556674	63.698356
1764.518803	24.247612	63.703361
1763.690485	30.142925	63.708366
1762.966250	22.012297	63.713370
1762.281592	26.065022	63.718375
1761.465696	19.379225	63.723380
1761.214442	20.415845	63.728385
1760.255396	21.667373	63.733390
1759.843604	14.069016	63.738394
1759.030213	22.265844	63.743399
1758.823620	29.027499	63.748404
1758.591948	20.925878	63.753409
1757.690599	25.582288	63.758414
1756.449586	26.842328	63.763418
1755.383326	25.160456	63.768423
1754.792807	29.050002	63.773428
1754.574975	21.755147	63.778433
1753.560359	24.559312	63.783438
1753.199373	17.126348	63.788442
1752.240802	27.689549	63.793447
1751.941805	33.926572	63.798452
1751.426507	14.039901	63.803457
1750.537940	16.190123	63.808462
1750.364309	19.046804	63.813466
1749.652877	22.094551	63.818471
1749.036682	18.281740	63.823476
1748.029837	18.079053	63.828481
1747.102628	18.488182	63.833486
1746.405106	19.762833	63.838490
1745.685081	23.422216	63.843495
1745.076596	17.282217	63.848500
1744.839509	26.748410	63.853505
1744.069633	27.597745	63.858510
1743.928081	12.954923	63.863514
1743.140895	26.982217	63.868519
1742.276024	21.291360	63.873524
1741.294535	10.725831	63.878529
1740.359869	28.097552	63.883534
1739.719714	23.340815	63.888538
1739.139144	17.229500	63.893543
1738.547708	23.233849	63.898548
1738.198913	19.774380	63.903553
1737.790367	14.818439	63.908558
1737.663963	11.434037	63.913562
1736.618880	18.923358	63.918567
1735.656807	11.954867	63.923572
1735.024260	10.005430	63.928577
1734.137781	24.072146	63.933582
1733.903925	20.586538	63.938586
1732.417777	22.986216	63.943591
1731.483069	12.528375	63.948596
1732.235861	22.610042	63.953601
1730.970491	35.620484	63.958606
1730.085003	23.352392	63.963610
1729.376421	25.344729	63.968615
1728.796875	14.638095	63.973620
1728.526106	11.756007	63.978625
1727.584270	28.927024	63.983630
1727.327002	26.110596	63.988634
1726.023104	22.949478	63.993639
1725.255814	20.037441	63.998644
1724.712909	20.991079	64.003649
1724.042741	17.049656	64.008654
1723.824043	14.249182	64.013658
1723.406212	23.425541	64.018663
1722.573786	14.769653	64.023668
1721.629323	9.245988	64.028673
1720.409646	23.425551	64.033678
1719.667448	18.601452	64.038682
1719.418341	17.120964	64.043687
1719.384697	16.218100	64.048692
1718.657803	15.573576	64.053697
1717.930821	12.579449	64.058702
1717.601756	15.364625	64.063706
1716.253230	21.516033	64.068711
1715.258214	22.396405	64.073716
1714.704630	12.234424	64.078721
1713.981766	24.791272	64.083726
1713.513999	15.170737	64.088730
1712.898833	21.232474	64.093735
1712.526798	20.131050	64.098740
1712.231033	19.110550	64.103745
1711.815668	23.979938	64.108750
1711.093089	23.072960	64.113754
1709.787663	16.237860	64.118759
1709.327474	21.890213	64.123764
1708.637866	23.890580	64.128769
1707.442444	18.895625	64.133774
1706.546334	19.217828	64.138778
1706.503995	27.142394	64.143783
1705.812369	16.679069	64.148788
1705.451690	25.754891	64.153793
1704.629500	34.080866	64.158798
1704.133934	19.379160	64.163802
1703.568456	26.683510	64.168807
1702.565859	23.644855	64.173812
1701.779920	23.072791	64.178817
1700.805630	16.949908	64.183822
1700.526691	14.717237	64.188826
1700.100467	19.928964	64.193831
1699.487773	27.305469	64.198836
1699.018705	17.243604	64.203841
1697.491088	16.516538	64.208846
1696.827554	15.775225	64.213850
1696.238594	12.700836	64.218855
1695.640279	19.452168	64.223860
1695.622323	15.924389	64.228865
1694.917961	26.082955	64.233870
1694.753837	17.125387	64.238874
1693.414542	14.594372	64.243879
1692.400810	16.105341	64.248884
1692.135172	13.635596	64.253889
1691.129296	24.392401	64.258894
1691.026838	10.899269	64.263898
1689.916107	13.945799	64.268903
1688.907413	15.320353	64.273908
1688.306207	14.688988	64.278913
1687.719724	20.347211	64.283918
1687.343663	16.124121	64.288922
1686.936879	24.264266	64.293927
1686.547109	20.924853	64.298932
1685.904858	12.256120	64.303937
1684.601103	15.055774	64.308942
1684.050119	11.084394	64.313946
1683.454952	13.143880	64.318951
1683.109545	22.165236	64.323956
1682.138045	21.956960	64.328961
1681.067122	20.115015	64.333966
1680.540756	15.537339	64.338970
1679.794046	14.763512	64.343975
1679.254784	23.516046	64.348980
1678.946254	5.892575	64.353985
1678.381407	21.715363	64.358990
1678.201031	15.035883	64.363994
1677.077543	11.459790	64.368999
1676.122263	17.816826	64.374004
1675.295421	17.289113	64.379009
1674.893117	16.829581	64.384014
1674.036024	22.368369	64.389018
1673.016197	15.300270	64.394023
1672.340197	19.949292	64.399028
1671.900315	11.177458	64.404033
1671.399127	21.333713	64.409038
1670.790139	13.960663	64.414042
1670.585715	10.792083	64.419047
1670.139111	13.455588	64.424052
1669.641603	7.479334	64.429057
1668.247246	13.535540	64.434062
1667.850055	4.116699	64.439066
1666.999913	11.619226	64.444071
1666.215440	7.885210	64.449076
1665.733170	10.538612	64.454081
1664.986679	18.253332	64.459086
1664.920801	19.597975	64.464090
1663.821219	16.008629	64.469095
1662.729968	16.590498	64.474100
1662.370298	10.007311	64.479105
1661.303662	24.894275	64.484110
1661.058836	5.276920	64.489114
1660.532494	10.720590	64.494119
1659.710451	19.839737	64.499124
1658.738268	18.426809	64.504129
1657.742272	13.952126	64.509134
1657.763382	0.338458	64.514138
1657.147153	11.484365	64.519143
1656.544724	14.155279	64.524148
1656.150049	8.432347	64.529153
1655.043110	11.743211	64.534158
1654.480394	14.538701	64.539162
1653.727523	23.309401	64.544167
1653.500617	8.877278	64.549172
1652.467746	13.720184	64.554177
1651.202476	15.853010	64.559182
1650.941926	10.143464	64.564186
1650.259761	18.079776	64.569191
1649.936953	27.781931	64.574196
1650.062454	27.514519	64.579201
1648.743452	20.984378	64.584206
1648.071087	17.816019	64.589210
1647.261484	27.461465	64.594215
1646.446467	23.566727	64.599220
1645.401440	17.079798	64.604225
1644.425045	20.954969	64.609230
1644.282653	17.070074	64.614234
1643.810319	21.560595	64.619239
1643.046127	18.987132	64.624244
1643.052490	9.694994	64.629249
1642.416256	25.770398	64.634254
1641.467244	21.122679	64.639258
1640.704698	15.453455	64.644263
1640.105396	12.871146	64.649268
1639.382110	20.430802	64.654273
1637.956534	17.695908	64.659278
1637.790019	14.330501	64.664282
1637.185789	14.262590	64.669287
1636.585000	9.606866	64.674292
1636.338927	13.695595	64.679297
1635.553496	23.480702	64.684302
1634.663119	27.616598	64.689306
1633.921124	19.447840	64.694311
1633.274353	14.269573	64.699316
1633.035823	9.423840	64.704321
1631.126345	19.201435	64.709326
1630.685708	17.986346	64.714330
1630.598105	10.640866	64.719335
1630.213025	17.831410	64.724340
1629.733488	6.590120	64.729345
1629.069687	11.088980	64.734350
1628.231831	10.894186	64.739354
1627.336484	11.446525	64.744359
1626.662507	13.362427	64.749364
1626.266930	18.455755	64.754369
1625.394847	17.952592	64.759374
1624.455960	11.808352	64.764378
1623.864719	22.592340	64.769383
1623.323037	21.666112	64.774388
1623.062947	17.203841	64.779393
1622.371818	19.664931	64.784398
1621.605568	12.308996	64.789402
1620.641391	15.942541	64.794407
1619.758674	25.391453	64.799412
1619.946805	15.308783	64.804417
1618.367059	21.556891	64.809422
1617.399918	9.210375	64.814426
1617.300834	10.576063	64.819431
1616.915928	13.209274	64.824436
1616.374560	20.546072	64.829441
1615.527694	21.068636	64.834446
1615.324182	10.430035	64.839450
1614.248806	19.214130	64.844455
1613.104236	22.885799	64.849460
1612.947658	16.314508	64.854465
1612.009703	15.719314	64.859470
1611.934820	12.107545	64.864474
1610.926515	12.498067	64.869479
1610.299467	21.707669	64.874484
1609.963958	16.621882	64.879489
1608.990150	23.163230	64.884494
1608.093096	12.822466	64.889498
1607.276007	18.626146	64.894503
1606.889167	8.078174	64.899508
1606.724199	8.637484	64.904513
1605.361430	19.963508	64.909518
1604.715878	17.486324	64.914522
1603.963113	7.240912	64.919527
1603.691074	14.105997	64.924532
1603.215690	20.319006	64.929537
1602.494527	19.977950	64.934542
1601.675184	16.200610	64.939546
1600.730469	17.886724	64.944551
1600.430629	12.216543	64.949556
1600.000591	3.785360	64.954561
1598.698487	15.231052	64.959566
1598.151237	9.221719	64.964570
1597.514264	10.570364	64.969575
1597.101925	5.153021	64.974580
1596.916239	13.516654	64.979585
1595.522394	21.752122	64.984590
1594.740223	14.518573	64.989594
1594.057288	12.849985	64.994599
1593.341038	20.045840	64.999604
1593.328926	18.868328	65.004609
1592.752827	17.466613	65.009614
1592.029988	14.156482	65.014618
1591.296386	16.599097	65.019623
1590.652405	10.598825	65.024628
1589.644642	20.340416	65.029633
1588.304609	26.662419	65.034638
1588.406044	16.809561	65.039642
1587.669042	11.388608	65.044647
1587.191734	13.765272	65.049652
1587.040134	9.634272	65.054657
1585.635439	20.793504	65.059662
1585.194232	16.311130	65.064666
1584.736604	16.213632	65.069671
1583.931023	15.346686	65.074676
1583.249669	9.500586	65.079681
1582.036650	20.988904	65.084686
1581.660599	8.488572	65.089690
1581.209938	14.000654	65.094695
1580.774411	18.326065	65.099700
1580.756701	15.072636	65.104705
1579.208194	13.166269	65.109710
1578.671719	12.065763	65.114714
1577.686633	23.601446	65.119719
1576.502725	9.690392	65.124724
1576.259964	8.297220	65.129729
1575.233331	11.382472	65.134734
1575.358624	11.952435	65.139738
1574.755292	17.764737	65.144743
1574.221433	19.559044	65.149748
1573.240411	9.457140	65.154753
1572.123907	15.209054	65.159758
1571.674941	10.125533	65.164762
1571.352164	19.428718	65.169767
1570.848316	10.551959	65.174772
1570.573827	0.728881	65.179777
1569.615308	18.679985	65.184782
1568.682551	29.903016	65.189786
1568.314548	11.473753	65.194791
1566.997526	12.428995	65.199796
1566.546846	9.346862	65.204801
1565.804084	7.859674	65.209806
1565.650423	3.161313	65.214810
1564.804732	18.517804	65.219815
1563.779152	20.756087	65.224820
1563.277670	-4.705517	65.229825
1562.912996	22.149142	65.234830
1562.262481	6.995889	65.239834
1560.599803	13.189394	65.244839
1559.959946	25.997999	65.249844
1559.749479	2.423453	65.254849
1559.313482	10.044702	65.259854
1558.712404	5.715469	65.264858
1558.456327	16.473014	65.269863
1557.629766	18.435254	65.274868
1556.811788	9.884373	65.279873
1555.771485	22.720334	65.284878
1555.248815	11.396032	65.289882
1554.867780	5.316149	65.294887
1554.382361	18.909169	65.299892
1553.514937	16.995522	65.304897
1552.656381	12.830200	65.309902
1552.395995	8.397951	65.314906
1551.691702	11.460379	65.319911
1550.724747	10.715278	65.324916
1549.863657	9.795664	65.329921
1549.184097	20.734038	65.334926
1548.725064	1.830412	65.339930
1548.469692	9.063424	65.344935
1547.179597	3.657832	65.349940
1546.689505	10.708948	65.354945
1546.103714	18.696196	65.359950
1545.705263	22.897453	65.364954
1545.448559	12.905969	65.369959
1544.151296	19.024077	65.374964
1543.568769	12.766478	65.379969
1542.600863	32.176170	65.384974
1542.327032	9.644571	65.389978
1541.628545	6.470935	65.394983
1540.589314	14.124962	65.399988
1540.145389	6.527038	65.404993
1539.408173	12.994540	65.409998
1539.105424	7.586603	65.415002
1538.602825	16.866322	65.420007
1537.540159	17.839509	65.425012
1537.122854	13.386463	65.430017
1536.293843	11.801027	65.435022
1535.788400	14.227901	65.440026
1534.741021	12.562048	65.445031
1534.170908	21.084538	65.450036
1534.217640	10.857189	65.455041
1532.949920	24.528792	65.460046
1532.005328	11.828658	65.465050
1531.595822	4.900189	65.470055
1530.798620	15.396795	65.475060
1530.358412	13.390041	65.480065
1529.983411	13.173770	65.485070
1528.934106	12.008110	65.490074
1528.218097	4.439231	65.495079
1527.564889	8.516967	65.500084
1527.429131	-1.511067	65.505089
1526.352230	14.328432	65.510094
1525.334114	8.168441	65.515098
1524.738633	-2.556078	65.520103
1524.261364	24.300701	65.525108
1524.121791	7.640736	65.530113
1523.468821	12.008589	65.535118
1522.594594	11.379648	65.540122
1522.025379	4.336215	65.545127
1520.729980	16.031601	65.550132
1520.106000	11.266057	65.555137
1519.498459	14.502348	65.560142
1519.175840	15.053600	65.565146
1518.558050	14.579449	65.570151
1518.032348	11.788362	65.575156
1517.258476	10.025440	65.580161
1516.295876	16.702224	65.585166
1515.930514	16.217924	65.590170
1515.464117	14.229527	65.595175
1514.595342	9.761498	65.600180
1513.801048	-0.764272	65.605185
1513.169683	14.398895	65.610190
1512.448396	16.191459	65.615194
1512.033255	7.335315	65.620199
1510.850456	14.321476	65.625204
1510.924323	0.218485	65.630209
1510.250134	7.650511	65.635214
1509.326573	11.123099	65.640218
1508.245154	4.220986	65.645223
1507.766679	5.672196	65.650228
1507.241539	11.404274	65.655233
1506.818007	6.592689	65.660238
1506.184803	10.932174	65.665242
1505.203107	8.789128	65.670247
1504.339637	8.175831	65.675252
1504.299282	4.486046	65.680257
1502.937629	-4.240177	65.685262
1502.302535	6.714781	65.690266
1501.681946	9.352343	65.695271
1501.159219	0.289380	65.700276
1501.075466	0.277561	65.705281
1500.122498	5.565126	65.710286
1499.257964	2.887812	65.715290
1499.075597	5.171889	65.720295
1498.286095	10.488672	65.725300
1497.285680	2.651195	65.730305
1496.590206	9.531532	65.735310
1496.075810	6.497385	65.740314
1495.435995	7.270930	65.745319
1494.310117	2.714462	65.750324
1493.724501	-1.027439	65.755329
1492.822255	8.181750	65.760334
1492.660068	7.214166	65.765338
1492.364384	4.293495	65.770343
1491.584782	3.979104	65.775348
1490.745285	-7.999694	65.780353
1489.819237	11.231442	65.785358
1489.840367	-4.295004	65.790362
1489.065546	8.030427	65.795367
1487.800996	10.688328	65.800372
1487.326351	-0.384959	65.805377
1486.879378	9.928263	65.810382
1486.234528	5.360008	65.815386
1485.042811	10.050023	65.820391
1484.161992	11.085794	65.825396
1484.038434	3.744472	65.830401
1483.498551	8.362437	65.835406
1483.338897	11.642672	65.840410
1482.423366	10.047350	65.845415
1481.195288	10.293079	65.850420
1480.810805	2.299380	65.855425
1480.388034	10.733801	65.860430
1479.524001	8.103722	65.865434
1478.552458	6.380111	65.870439
1477.905097	8.777510	65.875444
1477.786323	1.023854	65.880449
1477.292940	19.014592	65.885454
1476.305542	13.406393	65.890458
1475.681319	6.829021	65.895463
1474.722630	8.634090	65.900468
1474.338230	4.267294	65.905473
1473.241328	15.029154	65.910478
1472.860594	8.837277	65.915482
1472.370326	-2.071098	65.920487
1471.656180	9.082505	65.925492
1471.158721	-0.854922	65.930497
1470.190664	10.227073	65.935502
1469.391727	16.433171	65.940506
1469.045891	3.306766	65.945511
1468.349897	14.291913	65.950516
1467.458016	4.319397	65.955521
1466.846452	10.894675	65.960526
1466.436676	17.079926	65.965530
1466.098224	9.536218	65.970535
1465.042233	12.402252	65.975540
1464.589562	10.977799	65.980545
1463.682023	16.076814	65.985550
1462.676057	0.272063	65.990554
1461.865802	1.969970	65.995559
1461.133713	11.223088	66.000564
1461.177941	4.758678	66.005569
1460.391016	2.151044	66.010574
1459.996225	5.520687	66.015578
1459.451071	4.612393	66.020583
1458.333934	10.216217	66.025588
1457.965115	2.169573	66.030593
1456.858046	4.949113	66.035598
1456.051483	4.826671	66.040602
1455.655278	10.356919	66.045607
1455.035071	18.936263	66.050612
1455.046315	-0.232872	66.055617
1453.848496	9.141572	66.060622
1453.213662	15.693745	66.065626
1452.742184	12.414671	66.070631
1451.177158	7.904363	66.075636
1450.935975	18.106041	66.080641
1450.051632	18.603077	66.085646
1449.780515	13.347818	66.090650
1449.392348	7.966087	66.095655
1448.542095	13.295693	66.100660
1448.069959	11.036992	66.105665
1447.225485	2.657525	66.110670
1446.798012	14.645495	66.115674
1445.976788	7.041329	66.120679
1444.810632	15.098752	66.125684
1444.491477	4.459645	66.130689
1443.961684	13.258002	66.135694
1443.007472	14.814796	66.140698
1442.751178	8.219957	66.145703
1441.768225	8.040400	66.150708
1441.406994	13.383746	66.155713
1440.605685	17.228003	66.160718
1439.600618	11.485437	66.165722
1439.210687	12.542549	66.170727
1438.470313	13.431436	66.175732
1438.352498	11.723537	66.180737
1437.274580	9.042313	66.185742
1436.235573	6.982519	66.190746
1435.733367	12.499656	66.195751
1435.248579	14.585803	66.200756
1435.093475	10.436453	66.205761
1433.703231	8.831445	66.210766
1433.279144	12.648863	66.215770
1432.596721	7.061598	66.220775
1432.164112	8.284763	66.225780
1431.521803	2.112395	66.230785
1430.483213	20.582442	66.235790
1430.048821	5.282934	66.240794
1429.549726	7.360317	66.245799
1428.189633	11.654504	66.250804
1427.909445	15.245629	66.255809
1427.014926	13.388373	66.260814
1426.922416	8.100001	66.265818
1426.290208	17.062870	66.270823
1425.080525	17.487047	66.275828
1424.746724	12.356871	66.280833
1424.295925	13.258083	66.285838
1423.844541	17.529264	66.290842
1422.699041	4.496857	66.295847
1421.550909	25.868506	66.300852
1421.444949	16.147971	66.305857
1420.746466	13.888982	66.310862
1419.967919	13.825176	66.315866
1419.584989	3.738673	66.320871
1419.013873	17.591317	66.325876
1418.447071	7.540345	66.330881
1417.359977	9.689112	66.335886
1416.724105	14.342846	66.340890
1416.178999	12.378018	66.345895
1415.329762	16.474322	66.350900
1414.714684	7.006600	66.355905
1413.961779	12.189858	66.360910
1413.461880	13.090991	66.365914
1413.412499	11.952522	66.370919
1412.327278	18.768674	66.375924
1411.187591	10.101834	66.380929
1410.868109	2.558281	66.385934
1410.336771	10.787618	66.390938
1409.455368	7.841787	66.395943
1408.477160	17.578730	66.400948
1407.926306	10.105064	66.405953
1407.476297	14.234105	66.410958
1407.012553	9.398971	66.415962
1406.238027	10.804217	66.420967
1405.431103	7.953781	66.425972
1405.286551	7.096938	66.430977
1404.506159	6.858392	66.435982
1403.641260	13.701025	66.440986
1402.803744	10.079607	66.445991
1401.999777	9.601963	66.450996
1402.052232	-1.288580	66.456001
1400.995814	12.265893	66.461006
1399.989522	13.157636	66.466010
1399.890456	4.185053	66.471015
1398.884151	13.172695	66.476020
1398.224768	-2.253454	66.481025
1397.477293	18.409545	66.486030
1397.203578	13.528438	66.491034
1396.603820	7.022893	66.496039
1395.436737	5.325667	66.501044
1394.885718	5.004933	66.506049
1393.971474	11.025952	66.511054
1393.698357	10.210047	66.516058
1393.249920	6.444788	66.521063
1392.039515	5.919791	66.526068
1391.568405	7.361966	66.531073
1391.167371	10.559149	66.536078
1390.696503	23.424485	66.541082
1389.586668	18.179553	66.546087
1388.437714	18.876362	66.551092
1388.148093	8.968993	66.556097
1387.898140	10.910589	66.561102
1387.263025	11.517837	66.566106
1386.824446	18.278518	66.571111
1385.732944	21.899266	66.576116
1385.354545	14.396615	66.581121
1383.878411	14.051053	66.586126
1383.205946	11.734325	66.591130
1382.993809	15.935942	66.596135
1382.704770	16.948640	66.601140
1382.332580	14.938987	66.606145
1381.324332	11.556023	66.611150
1380.167206	11.093524	66.616154
1380.243923	11.808390	66.621159
1379.046384	19.872405	66.626164
1378.398344	6.631638	66.631169
1377.701517	8.395117	66.636174
1377.051938	15.484222	66.641178
1377.148388	4.905220	66.646183
1375.703790	7.148679	66.651188
1375.429741	-5.845602	66.656193
1374.526297	11.295698	66.661198
1373.272748	19.948924	66.666202
1372.983418	2.207387	66.671207
1372.308120	4.883632	66.676212
1372.079453	8.107033	66.681217
1371.598845	6.056272	66.686222
1370.774586	-0.612265	66.691226
1370.494823	-4.312867	66.696231
1369.324471	7.339037	66.701236
1368.493691	3.748102	66.706241
1367.539397	3.735902	66.711246
1367.049121	5.815048	66.716250
1366.866345	-0.942845	66.721255
1365.723999	17.313474	66.726260
1365.092183	11.836454	66.731265
1364.723836	10.896921	66.736270
1364.302753	9.240389	66.741274
1363.568269	12.973120	66.746279
1362.150313	9.790909	66.751284
1361.731020	-0.146296	66.756289
1361.220607	10.148635	66.761294
1360.530696	13.967319	66.766298
1360.474384	13.437067	66.771303
1359.005257	15.279167	66.776308
1358.542057	4.286097	66.781313
1357.873246	5.922127	66.786318
1357.804961	3.690709	66.791322
1356.719601	-7.849984	66.796327
1356.081488	-0.002633	66.801332
1355.366810	-0.168034	66.806337
1354.341154	-2.302452	66.811342
1353.696343	8.269303	66.816346
1353.368198	5.374313	66.821351
1352.828761	13.182331	66.826356
1352.641530	0.182133	66.831361
1351.458778	2.322479	66.836366
1350.481565	7.448370	66.841370
1349.931599	4.563412	66.846375
1349.568017	8.866373	66.851380
1349.042295	3.978030	66.856385
1348.257060	15.278573	66.861390
1347.549761	13.295392	66.866394
1347.027986	8.639805	66.871399
1345.871012	15.820615	66.876404
1345.449499	6.842529	66.881409
1344.881433	5.368636	66.886414
1344.109494	6.478605	66.891418
1343.352144	10.915126	66.896423
1342.788627	6.281946	66.901428
1342.597699	2.004265	66.906433
1341.403524	0.500601	66.911438
1340.497723	12.242923	66.916442
1340.166168	2.162467	66.921447
1339.817674	4.725268	66.926452
1339.204824	4.795989	66.931457
1338.165136	-2.557360	66.936462
1337.393717	9.603557	66.941466
1337.081922	2.456180	66.946471
1336.167645	8.483528	66.951476
1335.434679	5.181398	66.956481
1334.787588	1.357851	66.961486
1333.818483	-1.903582	66.966490
1333.618099	0.104252	66.971495
1332.802196	0.339717	66.976500
1332.289424	6.929271	66.981505
1331.865550	2.210818	66.986510
1330.914041	2.079921	66.991514
1329.870107	-6.184205	66.996519
1329.212062	4.768114	67.001524
1328.942477	3.756118	67.006529
1328.798106	0.267380	67.011534
1327.872336	0.231737	67.016538
1327.301172	-7.599780	67.021543
1326.281468	5.124143	67.026548
1325.966248	-4.235098	67.031553
1324.963467	0.223098	67.036558
1323.919814	-5.298814	67.041562
1323.726550	2.682821	67.046567
1323.224380	5.657976	67.051572
1322.118004	0.953416	67.056577
1321.397449	-3.060292	67.061582
1320.908781	-3.170154	67.066586
1320.932667	-0.573516	67.071591
1320.053267	-0.111915	67.076596
1319.036339	-3.912927	67.081601
1318.282017	-1.998372	67.086606
1317.464517	1.414836	67.091610
1316.333826	4.483609	67.096615
1315.851156	10.191615	67.101620
1315.282729	0.770130	67.106625
1314.932983	3.465593	67.111630
1314.719937	8.581966	67.116634
1314.442476	8.386489	67.121639
1313.428243	13.582933	67.126644
1312.776796	18.376356	67.131649
1311.784229	-1.796920	67.136654
1310.651737	0.352799	67.141658
1309.942173	-0.387400	67.146663
1309.435441	11.436558	67.151668
1309.304705	5.917738	67.156673
1309.044234	7.272823	67.161678
1307.974792	8.152564	67.166682
1307.402987	11.337485	67.171687
1306.479976	10.437261	67.176692
1306.125440	3.066455	67.181697
1304.930658	2.340325	67.186702
1304.408710	11.829715	67.191706
1304.107200	14.629473	67.196711
1302.969066	13.023878	67.201716
1302.456857	5.288642	67.206721
1301.655225	8.355566	67.211726
1301.058946	12.708144	67.216730
1300.897301	3.824369	67.221735
1299.732795	9.363245	67.226740
1299.443063	3.010287	67.231745
1298.972653	2.009723	67.236750
1298.172967	12.076268	67.241754
1297.499023	5.814357	67.246759
1296.503552	11.285360	67.251764
1296.032711	0.414949	67.256769
1295.134475	4.241537	67.261774
1294.145483	11.078697	67.266778
1294.205354	0.056101	67.271783
1293.159826	5.785791	67.276788
1292.646156	2.798885	67.281793
1291.759548	15.074320	67.286798
1290.943285	3.213333	67.291802
1290.628907	-3.577239	67.296807
1290.142873	-5.034198	67.301812
1289.620644	-3.093460	67.306817
1289.109073	-1.182800	67.311822
1288.076925	2.928426	67.316826
1287.121684	7.049502	67.321831
1285.952271	10.282136	67.326836
1285.532621	6.818246	67.331841
1285.358743	5.340039	67.336846
1285.147535	13.937953	67.341850
1284.838650	6.282355	67.346855
1283.630833	6.990146	67.351860
1282.796770	-3.858776	67.356865
1281.699567	4.681312	67.361870
1281.101459	9.456796	67.366874
1280.407302	6.676781	67.371879
1280.014607	18.179847	67.376884
1279.878660	4.485549	67.381889
1278.772056	11.809757	67.386894
1278.006627	16.632348	67.391898
1277.473128	1.630923	67.396903
1277.004234	6.502554	67.401908
1276.253602	9.991874	67.406913
1275.421227	7.807834	67.411918
1274.815350	16.958922	67.416922
1274.393262	11.043316	67.421927
1273.131902	4.390699	67.426932
1272.419613	7.452887	67.431937
1272.244116	9.693305	67.436942
1271.357000	21.076296	67.441946
1271.298877	-0.824028	67.446951
1269.875418	13.824874	67.451956
1269.554842	6.582712	67.456961
1269.433478	4.276161	67.461966
1268.252154	3.470639	67.466970
1267.528916	-1.007815	67.471975
1266.600240	17.613514	67.476980
1266.132601	10.104583	67.481985
1264.924586	10.741453	67.486990
1264.263691	2.307644	67.491994
1264.102093	2.716630	67.496999
1263.526883	5.137296	67.502004
1263.190348	4.746219	67.507009
1262.759779	7.397770	67.512014
1261.456976	4.206771	67.517018
1261.249158	2.145774	67.522023
1260.384145	4.312907	67.527028
1259.833864	-0.029047	67.532033
1258.802490	5.718905	67.537038
1258.127552	8.071853	67.542042
1257.969584	6.709387	67.547047
1257.028177	7.535676	67.552052
1256.342825	2.753163	67.557057
1255.665475	5.062341	67.562062
1254.947079	6.359359	67.567066
1254.026983	9.009905	67.572071
1252.995672	4.192519	67.577076
1253.053580	5.414983	67.582081
1252.690056	3.198977	67.587086
1251.647631	7.800695	67.592090
1251.094683	-1.743074	67.597095
1250.398324	10.197770	67.602100
1249.755041	-1.268087	67.607105
1248.907285	2.746026	67.612110
1248.000503	7.592675	67.617114
1247.881537	1.061190	67.622119
1247.178435	13.947681	67.627124
1246.545453	-4.426700	67.632129
1245.744377	-3.570684	67.637134
1245.223567	5.768720	67.642138
1245.080597	4.011219	67.647143
1243.791136	5.645045	67.652148
1243.352243	-5.025427	67.657153
1242.517061	12.836729	67.662158
1241.297007	9.722467	67.667162
1241.144959	9.332017	67.672167
1240.222215	6.840669	67.677172
1240.104531	-3.480343	67.682177
1239.381471	-4.287759	67.687182
1238.224595	4.725444	67.692186
1237.841406	-6.671379	67.697191
1237.320719	11.821995	67.702196
1236.472712	10.755332	67.707201
1235.600112	2.348890	67.712206
1234.933708	2.477037	67.717210
1234.665039	-0.883120	67.722215
1233.798274	2.952675	67.727220
1233.506928	-2.600517	67.732225
1232.888646	-7.835219	67.737230
1231.477604	-4.587796	67.742234
1230.808321	-8.740509	67.747239
1230.109564	2.648793	67.752244
1229.733228	-3.606801	67.757249
1229.471383	1.916291	67.762254
1228.840570	7.020252	67.767258
1228.198360	-2.818390	67.772263
1227.080165	10.922566	67.777268
1226.632282	4.664153	67.782273
1226.554955	-1.113877	67.787278
1225.127590	10.854907	67.792282
1224.821000	-0.689712	67.797287
1224.078952	3.231907	67.802292
1222.823106	9.990100	67.807297
1222.363063	11.023699	67.812302
1221.536942	8.532762	67.817306
1221.354075	0.354105	67.822311
1220.767003	-3.762796	67.827316
1220.317678	2.725220	67.832321
1219.391599	1.161636	67.837326
1218.505890	12.162794	67.842330
1218.266241	-0.425348	67.847335
1217.279972	-6.793675	67.852340
1216.336391	-2.871546	67.857345
1216.402802	-3.403963	67.862350
1215.395670	8.848072	67.867354
1214.600015	1.766626	67.872359
1213.614054	8.598597	67.877364
1213.452072	11.537019	67.882369
1213.274734	5.528893	67.887374
1211.941245	11.755404	67.892378
1211.511038	6.665831	67.897383
1210.593872	9.033657	67.902388
1210.076519	4.041521	67.907393
1209.482107	9.880848	67.912398
1208.732660	9.031905	67.917402
1208.353395	1.108404	67.922407
1207.263065	-1.110281	67.927412
1206.377727	7.588524	67.932417
1205.831601	0.995667	67.937422
1205.417042	12.491169	67.942426
1205.292489	-9.054793	67.947431
1204.157906	3.780466	67.952436
1203.211709	3.749694	67.957441
1202.858299	1.275052	67.962446
1202.436003	7.780850	67.967450
1201.508805	2.521164	67.972455
1200.553444	10.209268	67.977460
1200.149868	5.087079	67.982465
1199.912658	4.339601	67.987470
1198.738338	6.215329	67.992474
1198.265727	12.785900	67.997479
1197.693090	6.769679	68.002484
1196.809658	4.000867	68.007489
1195.628026	15.755551	68.012494
1195.053881	13.897893	68.017498
1194.875172	-2.383606	68.022503
1194.444504	7.553311	68.027508
1193.677265	10.868679	68.032513
1193.146628	5.042895	68.037518
1192.233988	-0.501369	68.042522
1191.913476	-3.225662	68.047527
1190.791281	7.108228	68.052532
1190.002138	11.434729	68.057537
1189.571692	8.671147	68.062542
1189.069782	8.892992	68.067546
1188.177625	0.227913	68.072551
1187.242422	9.719958	68.077556
1186.821347	1.441997	68.082561
1186.571980	4.283932	68.087566
1185.762329	5.655404	68.092570
1184.897472	-10.277271	68.097575
1184.037232	-3.466868	68.102580
1183.666530	2.373152	68.107585
1183.407244	3.529367	68.112590
1182.532898	17.482290	68.117594
1181.895876	5.067732	68.122599
1181.031091	15.695000	68.127604
1179.917962	1.279368	68.132609
1179.342676	4.348174	68.137614
1178.731924	2.937878	68.142618
1178.639087	-1.591919	68.147623
1178.205514	8.487384	68.152628
1177.383254	0.549189	68.157633
1176.491738	17.658671	68.162638
1175.784724	12.244129	68.167642
1174.672656	1.860501	68.172647
1173.976521	4.749837	68.177652
1173.669405	1.610264	68.182657
1173.071100	14.822289	68.187662
1172.682493	18.728713	68.192666
1172.004491	13.358442	68.197671
1171.032059	8.203730	68.202676
1170.464749	11.009503	68.207681
1170.124821	4.338130	68.212686
1168.883226	11.921960	68.217690
1168.609132	0.258648	68.222695
1168.018503	13.020031	68.227700
1166.803338	4.119333	68.232705
1166.230277	-2.912340	68.237710
1165.482421	7.809866	68.242714
1165.561890	-5.731007	68.247719
1164.791942	18.032636	68.252724
1163.787689	5.436800	68.257729
1162.988917	12.820898	68.262734
1162.295796	10.614749	68.267738
1162.423733	7.232524	68.272743
1161.131103	-1.878192	68.277748
1160.581415	-4.655915	68.282753
1160.217366	6.678590	68.287758
1159.131104	5.687694	68.292762
1158.485229	0.660821	68.297767
1157.819054	9.678012	68.302772
1157.290382	3.563350	68.307777
1156.582286	5.513176	68.312782
1155.534585	7.442899	68.317786
1155.088151	-2.513584	68.322791
1154.692934	4.052563	68.327796
1154.359412	3.216332	68.332801
1153.625443	2.902672	68.337806
1152.926877	1.586773	68.342810
1151.978160	5.290551	68.347815
1150.767209	12.511555	68.352820
1150.242254	4.521353	68.357825
1150.338816	4.078754	68.362830
1149.343514	5.946531	68.367834
1148.746265	-2.716549	68.372839
1147.653246	10.383352	68.377844
1147.365331	-4.422118	68.382849
1147.093110	0.339402	68.387854
1145.786218	13.055440	68.392858
1145.060159	-7.223191	68.397863
1144.489802	4.696045	68.402868
1144.431170	1.625762	68.407873
1143.558121	1.600724	68.412878
1142.570927	8.593758	68.417882
1142.059090	0.590436	68.422887
1141.342041	5.078942	68.427892
1140.719464	-1.686235	68.432897
1140.176064	5.327673	68.437902
1139.336650	9.487145	68.442906
1138.828073	5.228472	68.447911
1138.004946	0.201414	68.452916
1137.204464	4.830920	68.457921
1136.944045	9.694643	68.462926
1136.216290	3.821381	68.467930
1135.544285	0.164278	68.472935
1134.598516	10.107437	68.477940
1133.845637	1.458076	68.482945
1133.717174	3.281021	68.487950
1132.743753	7.468116	68.492954
1131.913484	-6.494165	68.497959
1131.311304	2.336233	68.502964
1130.571132	-6.964832	68.507969
1130.434407	5.524084	68.512974
1129.492177	7.681464	68.517978
1128.782664	3.946751	68.522983
1128.284068	11.246842	68.527988
1127.946801	3.181064	68.532993
1127.095914	-0.546929	68.537998
1125.822419	12.621109	68.543002
1125.771055	-8.878126	68.548007
1124.761644	12.778999	68.553012
1123.848098	11.774838	68.558017
1123.474304	-4.696378	68.563022
1122.482475	4.585497	68.568026
1122.839165	1.237847	68.573031
1121.226968	9.486178	68.578036
1120.740455	6.567530	68.583041
1119.784788	9.375161	68.588046
1119.694519	5.351148	68.593050
1119.343118	0.778906	68.598055
1118.688135	9.218749	68.603060
1118.300381	7.112272	68.608065
1117.083182	8.772512	68.613070
1116.130581	7.591645	68.618074
1115.693528	-2.760547	68.623079
1115.069426	5.344808	68.628084
1114.135626	6.650896	68.633089
1113.179615	6.954447	68.638094
1112.676666	7.316817	68.643098
1113.051520	6.743220	68.648103
1111.683630	12.085869	68.653108
1110.776206	5.653006	68.658113
1110.313079	-5.404646	68.663118
1109.728327	1.305190	68.668122
1108.906920	-5.444117	68.673127
1108.203028	2.274971	68.678132
1107.467941	2.792536	68.683137
1107.262640	12.747228	68.688142
1106.288517	17.662980	68.693146
1105.726498	-1.999927	68.698151
1104.976746	2.186290	68.703156
1104.510116	13.798887	68.708161
1104.081539	-3.769026	68.713166
1102.584312	3.932758	68.718170
1102.307290	8.053243	68.723175
1101.580855	16.554921	68.728180
1101.633738	0.534640	68.733185
1100.545296	-9.449007	68.738190
1099.545750	6.822972	68.743194
1099.302526	-3.735084	68.748199
1098.644116	1.994594	68.753204
1097.549440	5.825683	68.758209
1096.876361	-4.581996	68.763214
1096.450102	-5.818195	68.768218
1096.342221	3.868689	68.773223
1094.962713	4.785224	68.778228
1094.247353	14.513554	68.783233
1094.154941	-3.568287	68.788238
1092.978535	9.026088	68.793242
1092.375411	0.975802	68.798247
1091.596835	1.905555	68.803252
1091.290923	5.270564	68.808257
1090.947200	5.268574	68.813262
1089.744414	13.311452	68.818266
1089.318687	8.208579	68.823271
1088.742446	3.394571	68.828276
1087.933781	7.859818	68.833281
1087.006374	3.473823	68.838286
1086.251307	5.965711	68.843290
1086.151214	3.862366	68.848295
1085.502886	7.409575	68.853300
1084.451016	4.099911	68.858305
1083.938899	-3.767732	68.863310
1083.262520	5.780933	68.868314
1082.801951	-5.914190	68.873319
1081.708575	-3.242332	68.878324
1081.107071	-3.769426	68.883329
1080.568448	8.121118	68.888334
1080.097073	6.622446	68.893338
1079.133877	1.463153	68.898343
1078.598410	1.155785	68.903348
1078.181914	2.542016	68.908353
1077.792426	1.998542	68.913358
1076.930646	7.203928	68.918362
1076.111238	-5.987368	68.923367
1074.923414	6.813827	68.928372
1074.355876	1.282521	68.933377
1073.767049	-7.881751	68.938382
1073.040498	3.497805	68.943386
1073.263215	-0.038266	68.948391
1072.355342	-7.259491	68.953396
1070.863464	-3.426706	68.958401
1070.592969	-3.528650	68.963406
1070.188469	15.611701	68.968410
1069.756776	-3.873229	68.973415
1068.648099	4.810677	68.978420
1067.921043	4.002369	68.983425
1067.618912	-0.139319	68.988430
1066.768610	13.142763	68.993434
1066.064818	4.947652	68.998439
1065.466623	3.223160	69.003444
1065.317902	14.797801	69.008449
1064.158617	13.582026	69.013454
1063.210829	10.618502	69.018458
1063.193985	-3.113614	69.023463
1062.132486	0.382635	69.028468
1061.238732	1.583026	69.033473
1060.793013	-1.558134	69.038478
1060.333656	-2.596678	69.043482
1059.661640	2.991674	69.048487
1058.454909	5.670537	69.053492
1057.964988	-2.263708	69.058497
1057.875535	-1.273268	69.063502
1056.512693	-1.507355	69.068506
1056.042097	-3.439795	69.073511
1055.435170	2.563968	69.078516
1054.861025	-8.300967	69.083521
1054.565435	-11.171124	69.088526
1053.183841	0.968635	69.093530
1052.599137	-1.309918	69.098535
1052.324726	5.814170	69.103540
1052.019139	0.774194	69.108545
1051.350715	-5.204664	69.113550
1050.016565	8.111814	69.118554
1049.870849	0.925459	69.123559
1048.514700	1.809918	69.128564
1047.643752	0.764318	69.133569
1047.789425	0.052135	69.138574
1047.004290	1.405556	69.143578
1046.843486	-2.096309	69.148583
1045.688158	3.923740	69.153588
1044.961253	1.213660	69.158593
1044.527372	-2.457644	69.163598
1042.865362	-0.870104	69.168602
1042.329086	-2.829939	69.173607
1041.697283	-3.590316	69.178612
1041.679733	-7.583312	69.183617
1041.434213	-4.603213	69.188622
1040.753256	6.628751	69.193626
1039.757101	2.950708	69.198631
1039.439419	1.430748	69.203636
1038.642236	-4.874543	69.208641
1037.472752	-2.050214	69.213646
1036.467883	5.655273	69.218650
1036.565346	0.015028	69.223655
1036.148887	-0.935721	69.228660
1035.210114	6.246755	69.233665
1034.640165	2.764252	69.238670
1033.890131	1.161693	69.243674
1033.006689	-0.608870	69.248679
1032.125219	7.633637	69.253684
1031.892657	-3.425982	69.258689
1031.282660	2.442659	69.263694
1029.692269	8.975045	69.268698
1029.425851	-5.841696	69.273703
1028.929997	5.272513	69.278708
1028.629077	6.233522	69.283713
1028.417170	-3.323433	69.288718
1027.020357	1.960779	69.293722
1026.662681	-3.875128	69.298727
1025.910770	-1.949837	69.303732
1024.972092	19.423255	69.308737
1024.605406	-8.014900	69.313742
1023.684566	12.327199	69.318746
1023.538901	4.489573	69.323751
1022.221258	-1.846445	69.328756
1021.339853	-1.639883	69.333761
1020.970311	-12.980465	69.338766
1020.370359	10.527472	69.343770
1020.248063	-5.491725	69.348775
1018.772280	0.177205	69.353780
1018.265597	3.012783	69.358785
1017.913329	-6.032994	69.363790
1017.289395	7.436998	69.368794
1017.151366	-1.442599	69.373799
1016.082164	3.748496	69.378804
1015.379564	-9.565428	69.383809
1014.339809	-5.050784	69.388814
1013.397496	4.628510	69.393818
1013.431363	-13.549083	69.398823
1012.793112	-0.624008	69.403828
1011.858356	-7.946582	69.408833
1011.034999	-1.566189	69.413838
1010.182086	3.210461	69.418842
1010.137263	-14.506768	69.423847
1009.666343	-5.189477	69.428852
1008.750157	-11.543626	69.433857
1007.940742	-8.938996	69.438862
1007.186234	-14.055763	69.443866
1006.506593	-2.705742	69.448871
1005.458094	-3.396658	69.453876
1004.952290	1.274305	69.458881
1004.719509	-5.051387	69.463886
1003.651928	1.542903	69.468890
1003.782718	-7.617572	69.473895
1003.083748	3.973643	69.478900
1002.426119	0.558714	69.483905
1001.751134	-9.336126	69.488910
1000.433322	1.604518	69.493914
999.765709	-9.548292	69.498919
999.378423	-6.285444	69.503924
999.031955	9.975688	69.508929
997.907704	-8.832905	69.513934
996.896367	-6.350681	69.518938
996.959660	-6.647647	69.523943
996.616602	5.692742	69.528948
995.297064	-2.325522	69.533953
994.578568	2.423437	69.538958
994.035631	-0.287512	69.543962
993.988053	-11.964737	69.548967
992.822662	-6.102338	69.553972
992.353114	3.080703	69.558977
991.989164	-2.386778	69.563982
990.380854	-5.122174	69.568986
990.003341	-12.915011	69.573991
989.371924	-5.232666	69.578996
988.823657	2.636720	69.584001
987.783579	-6.277534	69.589006
986.837578	1.224640	69.594010
986.511765	-10.051933	69.599015
986.318335	4.448666	69.604020
985.598375	1.592425	69.609025
985.408424	-8.348047	69.614030
984.329903	-2.267660	69.619034
983.657561	2.524419	69.624039
982.750802	1.325272	69.629044
982.054233	-2.928677	69.634049
981.555127	-2.710392	69.639054
981.139425	-4.552206	69.644058
980.605802	-2.123910	69.649063
979.523073	-4.450930	69.654068
978.769434	-10.026707	69.659073
978.391084	-5.989440	69.664078
977.563841	-0.218684	69.669082
976.799995	-8.866232	69.674087
976.110984	-7.209550	69.679092
975.906639	-3.360814	69.684097
974.896100	-6.788962	69.689102
974.033973	-5.025888	69.694106
973.672557	-4.980894	69.699111
973.473115	-7.935722	69.704116
972.451602	2.197717	69.709121
971.650289	0.273763	69.714126
970.885428	0.017110	69.719130
970.261160	-7.329619	69.724135
969.141127	-8.665130	69.729140
968.398459	3.234232	69.734145
968.314378	-5.062599	69.739150
967.818828	4.685963	69.744154
967.462445	-8.435457	69.749159
966.536098	-2.672583	69.754164
965.695344	-6.622893	69.759169
965.153823	-10.687046	69.764174
963.745037	-6.687658	69.769178
963.232769	-13.632746	69.774183
962.792318	-7.571885	69.779188
962.552923	-5.620900	69.784193
962.659922	-14.036437	69.789198
961.381569	-10.371607	69.794202
960.834641	-3.743461	69.799207
959.130993	-7.397194	69.804212
958.282247	-5.352401	69.809217
957.845800	-4.715163	69.814222
957.212013	-5.585586	69.819226
957.286681	-1.503710	69.824231
957.127984	-1.850506	69.829236
956.224376	-7.555372	69.834241
955.396788	-9.098257	69.839246
954.716541	4.793849	69.844250
954.099582	-7.328919	69.849255
953.478572	-2.798886	69.854260
952.549734	0.698373	69.859265
951.840175	-3.424193	69.864270
950.572140	5.781838	69.869274
950.007424	-1.998552	69.874279
949.615315	-4.197342	69.879284
949.472108	1.677456	69.884289
949.207559	-8.304753	69.889294
947.908864	9.058777	69.894298
947.547620	-8.363673	69.899303
946.604047	-3.500043	69.904308
945.244388	4.255621	69.909313
945.062131	0.058609	69.914318
944.363235	1.477183	69.919322
944.197795	-5.940974	69.924327
943.521018	-5.878907	69.929332
942.430500	5.279475	69.934337
942.149187	-2.158091	69.939342
941.322688	-2.128967	69.944346
940.314864	6.794395	69.949351
939.574840	0.085818	69.954356
939.146538	-8.436921	69.959361
939.041437	-10.821725	69.964366
937.924508	-5.343897	69.969370
937.649428	-14.791428	69.974375
936.550463	-5.601264	69.979380
935.942396	-1.396553	69.984385
934.917354	-9.601985	69.989390
934.096535	4.761912	69.994394
933.981317	-8.872524	69.999399
933.769889	-7.178293	70.004404
932.920674	-4.182541	70.009409
932.117480	-10.942558	70.014414
931.703251	-10.458657	70.019418
931.101328	-5.638353	70.024423
930.126851	-5.707099	70.029428
929.229575	-14.552582	70.034433
928.960289	-7.404082	70.039438
927.578651	-1.936162	70.044442
926.915706	-6.632247	70.049447
926.687454	0.169114	70.054452
926.116367	0.337365	70.059457
925.922543	-17.822894	70.064462
924.580205	-7.561124	70.069466
924.072663	-14.022842	70.074471
923.616249	-14.494141	70.079476
922.304476	-4.147348	70.084481
921.737673	-12.296388	70.089486
921.155303	-1.799172	70.094490
921.046797	-11.367825	70.099495
920.494176	-6.378751	70.104500
919.382627	-4.493967	70.109505
919.016291	-7.283462	70.114510
918.269635	-1.911858	70.119514
917.409445	-14.904197	70.124519
916.578719	-16.895987	70.129524
915.736961	1.542816	70.134529
915.734436	-7.260558	70.139534
915.118318	-8.024975	70.144538
913.926008	-16.607462	70.149543
913.215592	-6.761633	70.154548
912.934485	-7.000638	70.159553
912.604025	-11.579323	70.164558
911.363936	-5.222471	70.169562
911.011575	-6.900892	70.174567
910.386603	-13.996757	70.179572
909.495920	-7.906816	70.184577
909.034026	-8.654776	70.189582
908.303174	7.467255	70.194586
907.799718	3.561053	70.199591
906.772829	-8.939570	70.204596
905.975976	-3.436975	70.209601
905.778737	-4.632318	70.214606
905.339931	1.686904	70.219610
904.283257	-8.922995	70.224615
903.380963	-10.521779	70.229620
902.883546	-3.154050	70.234625
902.523700	-16.326930	70.239630
901.515433	-11.861412	70.244634
901.204834	-8.170801	70.249639
900.597526	-6.732100	70.254644
899.102217	-7.219401	70.259649
898.834113	-12.899227	70.264654
898.050240	2.674589	70.269658
898.163270	1.735788	70.274663
897.250156	1.758211	70.279668
896.125306	-3.110351	70.284673
895.483173	-12.530997	70.289678
895.068929	-6.292955	70.294682
894.322393	-9.558086	70.299687
893.729716	-3.663795	70.304692
892.744881	-3.084346	70.309697
892.829020	-9.698568	70.314702
892.083108	-8.327690	70.319706
891.097704	-9.957397	70.324711
890.414552	-12.813155	70.329716
890.011491	-4.955832	70.334721
888.978012	-19.008641	70.339726
888.023299	-7.775673	70.344730
887.788902	-10.108358	70.349735
887.442509	-2.195398	70.354740
886.259091	-4.722388	70.359745
885.830535	-7.039941	70.364750
885.186751	-0.287560	70.369754
884.681025	-10.512060	70.374759
883.519212	0.611954	70.379764
882.984263	-13.528084	70.384769
882.533760	-8.533180	70.389774
881.961153	-5.778550	70.394778
881.171872	-9.057373	70.399783
880.341940	-8.209268	70.404788
879.795109	-2.473654	70.409793
879.406663	-8.060210	70.414798
878.256977	-10.299258	70.419802
877.856402	0.643680	70.424807
876.927711	-0.861011	70.429812
876.506849	2.511272	70.434817
876.319125	-5.620822	70.439822
875.153162	-2.931020	70.444826
874.719148	-17.318922	70.449831
873.959655	4.162840	70.454836
872.926662	-11.058534	70.459841
872.426392	-7.850227	70.464846
871.697249	1.033528	70.469850
871.524429	-11.749657	70.474855
870.461578	-8.273621	70.479860
869.716714	-2.743023	70.484865
869.227318	-6.105840	70.489870
868.715982	-4.649292	70.494874
867.874200	-4.267638	70.499879
867.301271	-5.876254	70.504884
866.549163	-2.938514	70.509889
866.388192	-6.475025	70.514894
864.902260	-6.388228	70.519898
864.265225	-21.451839	70.524903
863.915494	-12.100215	70.529908
863.409073	-6.937141	70.534913
863.103330	-17.269150	70.539918
861.915979	-6.718217	70.544922
861.201384	-14.230297	70.549927
860.913880	-3.994467	70.554932
860.055249	-3.963356	70.559937
859.148601	-10.259036	70.564942
858.465503	-6.772476	70.569946
858.160012	-9.437607	70.574951
857.737083	-3.463098	70.579956
856.818566	-4.726556	70.584961
855.858360	-5.221733	70.589966
855.353693	-3.288440	70.594970
854.649224	-6.318987	70.599975
853.830302	-8.314212	70.604980
853.263615	-1.370676	70.609985
853.365482	-12.638016	70.614990
852.050386	1.295223	70.619994
851.126569	-6.708667	70.624999
850.726649	3.362141	70.630004
850.552159	-13.027160	70.635009
849.863428	-11.444605	70.640014
848.813614	-2.751075	70.645018
848.122924	-8.690051	70.650023
847.519190	-6.745720	70.655028
846.834038	-4.383164	70.660033
846.493427	-16.813213	70.665038
845.460495	-8.328946	70.670042
844.430406	-5.375339	70.675047
844.022876	-9.694171	70.680052
843.494440	-7.514250	70.685057
842.911307	-9.569077	70.690062
842.338105	-3.807184	70.695066
841.203901	3.098958	70.700071
840.598416	-1.524248	70.705076
840.319189	-7.470370	70.710081
839.976376	-3.564896	70.715086
838.458967	-7.858450	70.720090
838.141008	-20.599595	70.725095
838.001723	-8.755263	70.730100
836.843781	-9.070729	70.735105
836.145381	-23.621526	70.740110
835.121332	-0.676868	70.745114
835.058549	2.751962	70.750119
834.622598	-7.882587	70.755124
833.573137	-8.194819	70.760129
833.022589	-14.458861	70.765134
832.337707	-2.511911	70.770138
831.677385	-5.532131	70.775143
830.841955	-8.866667	70.780148
830.109254	-14.641257	70.785153
829.883942	-5.873964	70.790158
828.856357	-9.624177	70.795162
828.305282	-18.767562	70.800167
827.735753	1.289977	70.805172
827.120960	3.448957	70.810177
826.413758	-6.336615	70.815182
825.625685	0.165939	70.820186
825.252493	-6.675098	70.825191
824.603701	-11.051713	70.830196
823.517009	-1.781464	70.835201
822.722889	-8.330000	70.840206
822.211611	-12.255431	70.845210
821.951541	-5.165163	70.850215
821.042113	-14.890152	70.855220
820.171144	-6.281851	70.860225
820.014572	-6.517016	70.865230
819.216003	-8.763042	70.870234
818.007519	1.031207	70.875239
817.568546	-16.058705	70.880244
817.006778	-3.987852	70.885249
816.912928	-10.302512	70.890254
815.502915	-5.208479	70.895258
814.877700	-8.174360	70.900263
814.470505	-7.923365	70.905268
814.017150	1.736492	70.910273
813.055930	-2.320739	70.915278
811.959982	2.581384	70.920282
811.568783	-0.388634	70.925287
811.444930	-10.651821	70.930292
810.645437	0.931768	70.935297
810.219486	-4.968916	70.940302
808.918283	-0.336886	70.945306
808.619790	-1.699024	70.950311
807.524047	-0.756545	70.955316
806.870173	-7.187055	70.960321
806.375425	-16.301555	70.965326
806.091404	-11.169146	70.970330
805.736552	-12.363043	70.975335
804.532128	-15.951056	70.980340
803.945730	-12.184997	70.985345
803.341264	-13.156238	70.990350
802.074180	-4.533760	70.995354
801.441073	-7.801147	71.000359
801.268713	-10.020698	71.005364
800.505854	-8.150372	71.010369
800.461592	-11.759067	71.015374
799.179279	-4.726838	71.020378
798.714698	-6.390531	71.025383
798.093568	-8.018265	71.030388
796.834401	-2.669122	71.035393
796.565550	-15.552115	71.040398
795.967026	-8.184049	71.045402
795.405381	-12.222878	71.050407
794.705011	-9.872080	71.055412
793.983916	-0.819287	71.060417
793.389068	-8.884978	71.065422
792.788991	-6.553299	71.070426
791.995978	-5.857695	71.075431
791.143538	-4.045642	71.080436
790.615117	2.128590	71.085441
790.286193	-12.350132	71.090446
789.061103	-6.648454	71.095450
788.563636	-15.248445	71.100455
788.212164	-12.847535	71.105460
787.687315	3.989164	71.110465
786.552443	-3.457567	71.115470
785.356054	-1.668027	71.120474
785.159310	-5.198835	71.125479
785.166133	-4.687325	71.130484
784.190620	4.577858	71.135489
783.460583	-11.022842	71.140494
783.138400	6.303551	71.145498
782.306051	-6.183821	71.150503
781.183409	-1.214362	71.155508
780.425594	4.300975	71.160513
780.164526	0.673177	71.165518
779.691171	-2.419370	71.170522
778.819724	-6.271686	71.175527
778.099159	-0.363322	71.180532
777.652909	2.418522	71.185537
776.860296	1.407855	71.190542
775.775194	0.200908	71.195546
775.355360	-3.685457	71.200551
775.195213	-4.598119	71.205556
774.137118	-7.184425	71.210561
773.390978	-3.244699	71.215566
772.755756	-3.102472	71.220570
772.183062	-12.482090	71.225575
771.442465	-9.514620	71.230580
770.689410	-13.598661	71.235585
770.195709	-12.980661	71.240590
769.706839	-8.566244	71.245594
768.839462	1.271488	71.250599
768.004482	-4.623992	71.255604
767.404842	-6.490098	71.260609
767.431823	1.762386	71.265614
766.844476	-8.844887	71.270618
765.910501	-11.685907	71.275623
765.001948	-11.047592	71.280628
763.871106	-3.317239	71.285633
763.470133	-11.024289	71.290638
762.780448	-7.325353	71.295642
762.207641	-14.000557	71.300647
761.680349	-8.130847	71.305652
760.445274	-7.901004	71.310657
760.166016	-16.015346	71.315662
759.318268	-6.190203	71.320666
758.932652	-12.448944	71.325671
758.834815	-11.422470	71.330676
757.381555	-6.569097	71.335681
756.791438	-17.850834	71.340686
756.576861	-7.882074	71.345690
755.691716	-8.040666	71.350695
754.869118	-9.111204	71.355700
754.254355	-10.200638	71.360705
753.905691	-8.216473	71.365710
753.153247	-3.198712	71.370714
752.140161	-10.743655	71.375719
751.863484	3.188299	71.380724
750.976511	-0.327232	71.385729
750.511082	-9.097891	71.390734
749.338970	-2.862175	71.395738
749.006346	-7.874135	71.400743
748.799677	-2.459154	71.405748
747.492172	1.503724	71.410753
747.459969	-10.472371	71.415758
746.338567	-6.944388	71.420762
745.777925	-12.188118	71.425767
745.171086	-9.169399	71.430772
744.432874	-5.886920	71.435777
743.937503	-6.296791	71.440782
743.215668	-15.471309	71.445786
742.152468	-11.176755	71.450791
741.969041	-10.094078	71.455796
741.335525	-1.200293	71.460801
740.486080	-14.553792	71.465806
739.660212	-4.356824	71.470810
738.991451	-8.719195	71.475815
738.663319	-9.385920	71.480820
737.875993	-6.947148	71.485825
737.449383	-10.263161	71.490830
736.533092	-7.488476	71.495834
735.882597	-9.870009	71.500839
734.789898	-13.882616	71.505844
734.123109	-6.379096	71.510849
734.003104	-3.838417	71.515854
733.481878	-0.820709	71.520858
732.714509	-6.353212	71.525863
731.924933	-4.156924	71.530868
730.960030	-4.216078	71.535873
731.172895	-8.477548	71.540878
729.961442	-5.343639	71.545882
729.272069	-6.796491	71.550887
728.701017	-10.974149	71.555892
727.552813	-12.279833	71.560897
726.788375	-25.905460	71.565902
726.062347	-7.597031	71.570906
725.835341	-14.525970	71.575911
725.674149	-7.593365	71.580916
725.070189	-10.034342	71.585921
724.385624	-18.735406	71.590926
723.605300	-15.668562	71.595930
722.441314	-18.922359	71.600935
721.670259	-23.711543	71.605940
721.031362	-13.929111	71.610945
721.260481	-24.322587	71.615950
719.636495	-16.955239	71.620954
719.262715	-27.394642	71.625959
718.607725	-14.197230	71.630964
718.202126	-8.517195	71.635969
717.339770	-36.650496	71.640974
716.551692	-23.009293	71.645978
716.271941	-14.187608	71.650983
715.707745	-15.091124	71.655988
714.685507	-13.278821	71.660993
714.221381	-22.596854	71.665998
713.285823	-10.141640	71.671002
712.836159	-11.738306	71.676007
711.958162	-27.228668	71.681012
711.015197	-17.106095	71.686017
710.749974	-19.170506	71.691022
710.055530	-18.962065	71.696026
708.892019	-25.226236	71.701031
708.153566	-18.808831	71.706036
707.413878	-11.749427	71.711041
707.591302	-30.258871	71.716046
706.995049	-15.862906	71.721050
706.695269	-17.399859	71.726055
706.095660	-22.601101	71.731060
704.753361	-10.965765	71.736065
704.159317	-17.178689	71.741070
703.371268	-5.934365	71.746074
702.798042	-14.057081	71.751079
702.380691	-15.185819	71.756084
701.604784	-12.449245	71.761089
701.003155	-13.319989	71.766094
700.352259	-12.366297	71.771098
699.588144	-4.025706	71.776103
698.749109	-13.000203	71.781108
697.831300	-11.228174	71.786113
697.624426	-25.134950	71.791118
696.990689	-14.359888	71.796122
696.268280	-1.296803	71.801127
695.409911	-15.505116	71.806132
694.744315	-5.813037	71.811137
694.434737	-18.382021	71.816142
693.185676	-15.776679	71.821146
692.713752	-8.228489	71.826151
692.234748	-15.871057	71.831156
691.733396	-13.099351	71.836161
690.848084	-14.828488	71.841166
690.126385	-6.493074	71.846170
689.512614	-13.574881	71.851175
688.932870	-12.965242	71.856180
688.432867	-17.157354	71.861185
687.239234	-18.225557	71.866190
686.568234	-16.330403	71.871194
686.571439	-20.216299	71.876199
686.049237	-21.613757	71.881204
684.845503	-14.751685	71.886209
684.580826	-17.563631	71.891214
683.828661	-17.322339	71.896218
683.167556	-26.690994	71.901223
682.560156	-28.565300	71.906228
681.759370	-6.473014	71.911233
681.064269	-16.150065	71.916238
680.189250	-22.259893	71.921242
679.377100	-16.248625	71.926247
679.325970	-24.197428	71.931252
678.801259	-19.283724	71.936257
677.744285	-17.483221	71.941262
677.059063	-14.947155	71.946266
676.471102	-17.849543	71.951271
675.469100	-12.926064	71.956276
674.431201	-11.604821	71.961281
674.175967	-27.460826	71.966286
673.514566	-7.923239	71.971290
673.325980	-18.628660	71.976295
672.920450	-14.082427	71.981300
671.680284	-12.311095	71.986305
671.581906	-16.540349	71.991310
670.397575	-15.433900	71.996314
669.525732	-17.611437	72.001319
668.864214	-11.438075	72.006324
668.168529	-9.023338	72.011329
668.085833	-18.498290	72.016334
667.471682	-19.914217	72.021338
666.375041	-12.175086	72.026343
666.466584	-14.165420	72.031348
664.959712	-15.421845	72.036353
664.373723	-26.168052	72.041358
663.929091	-16.631006	72.046362
663.485537	-11.192496	72.051367
662.423820	-20.533623	72.056372
661.254186	-15.660714	72.061377
660.952464	-9.163034	72.066382
660.513932	-12.554401	72.071386
660.286091	-30.385888	72.076391
659.869813	-20.601056	72.081396
658.754700	-10.692317	72.086401
658.089911	-14.290496	72.091406
656.931204	-16.043891	72.096410
656.254535	-23.839465	72.101415
655.856236	-17.832594	72.106420
655.332642	-10.769744	72.111425
654.920971	-9.176067	72.116430
653.851313	-13.785219	72.121434
653.222557	-16.417763	72.126439
652.880311	-29.930818	72.131444
651.882524	-16.322432	72.136449
651.440509	-23.026311	72.141454
650.763494	-22.852167	72.146458
649.635058	-18.553499	72.151463
649.020580	-16.878642	72.156468
647.996855	-14.514160	72.161473
647.857854	-12.687947	72.166478
647.503915	-3.528022	72.171482
647.032520	-11.346827	72.176487
646.238409	-26.196099	72.181492
645.405866	-17.354190	72.186497
645.024561	-22.241683	72.191502
643.975038	-12.822764	72.196506
643.369144	-20.411993	72.201511
643.090067	-27.192276	72.206516
641.870795	-13.479231	72.211521
641.058934	-27.297533	72.216526
640.527817	-17.385603	72.221530
640.123029	-27.386398	72.226535
639.741699	-18.641575	72.231540
638.653260	-6.948869	72.236545
638.143177	-27.658983	72.241550
637.788953	-16.795968	72.246554
636.839446	-16.950575	72.251559
636.075992	-15.237798	72.256564
635.215248	-9.220353	72.261569
634.935020	-27.800406	72.266574
633.783105	-19.803315	72.271578
632.857548	-17.959070	72.276583
632.625386	-20.533344	72.281588
631.988663	-3.540067	72.286593
631.956995	-13.805287	72.291598
631.096042	-16.066543	72.296602
630.086001	-9.555404	72.301607
629.712588	-16.465741	72.306612
628.903827	-8.960093	72.311617
628.307603	-22.462662	72.316622
627.453148	-17.263054	72.321626
626.887588	-18.000757	72.326631
626.210596	-27.541896	72.331636
625.057775	-19.292353	72.336641
624.837611	-19.053768	72.341646
624.332055	-18.168934	72.346650
623.945659	-18.950938	72.351655
622.986251	-22.461185	72.356660
622.329372	-18.037338	72.361665
621.662848	-21.198426	72.366670
620.633581	-13.823236	72.371674
619.994028	-17.128964	72.376679
619.360429	-23.283522	72.381684
618.896123	-20.722703	72.386689
618.841505	-25.815176	72.391694
617.829930	-26.708918	72.396698
616.991713	-15.172753	72.401703
616.904422	-20.100757	72.406708
615.604002	-16.301370	72.411713
615.007785	-26.022521	72.416718
614.393530	-19.511338	72.421722
613.353623	-25.533378	72.426727
612.726629	-24.378474	72.431732
611.923713	-7.073313	72.436737
611.992089	-22.124586	72.441742
611.357918	-26.121849	72.446746
610.165093	-23.676808	72.451751
609.783875	-26.075957	72.456756
609.317932	-17.282965	72.461761
608.406031	-19.838862	72.466766
607.463707	-14.527486	72.471770
606.657187	-13.916403	72.476775
606.568160	-14.971261	72.481780
605.915555	-11.967301	72.486785
604.708744	-19.093396	72.491790
604.039706	-17.080267	72.496794
603.347236	-4.226936	72.501799
603.252266	-17.241647	72.506804
602.560340	-11.374079	72.511809
601.660705	-25.044348	72.516814
601.273905	-12.782161	72.521818
600.658957	-7.592303	72.526823
599.780260	-18.433796	72.531828
598.834601	-24.010384	72.536833
598.605136	-19.481147	72.541838
598.205182	-13.175971	72.546842
597.221825	-13.421363	72.551847
596.639494	-24.322666	72.556852
595.916600	-17.116109	72.561857
595.038426	-11.433334	72.566862
593.984112	-13.900316	72.571866
593.516650	-17.523594	72.576871
593.095894	-12.978080	72.581876
592.754274	-7.467490	72.586881
592.007156	-9.158678	72.591886
590.900979	-10.707526	72.596890
590.225715	-5.321984	72.601895
589.762040	-13.430575	72.606900
589.459040	-4.758139	72.611905
588.567219	-7.933798	72.616910
587.825404	-7.758778	72.621914
587.655065	-8.922107	72.626919
586.874482	-19.063306	72.631924
585.535560	-9.517852	72.636929
585.659194	-18.281357	72.641934
584.970988	-10.514212	72.646938
583.759129	-9.704526	72.651943
583.328081	-12.950416	72.656948
582.314505	-3.007358	72.661953
581.868001	-14.892207	72.666958
580.794750	-5.772249	72.671962
580.324942	-11.937118	72.676967
580.455068	-18.213307	72.681972
579.367749	-2.561160	72.686977
578.906101	-21.082348	72.691982
578.130227	-14.849756	72.696986
577.751929	-7.969303	72.701991
576.783149	-16.506777	72.706996
575.905666	-3.051559	72.712001
575.691024	-9.823177	72.717006
574.662929	-9.856437	72.722010
573.922966	-6.204640	72.727015
573.458165	-16.219519	72.732020
572.663620	-10.012335	72.737025
571.881192	-20.924337	72.742030
571.215917	-8.333949	72.747034
570.561906	-16.503677	72.752039
570.268599	-12.587143	72.757044
569.087331	-2.437604	72.762049
568.459929	-7.749497	72.767054
567.745587	-9.573627	72.772058
567.384293	-14.847480	72.777063
567.641780	-15.585381	72.782068
566.132514	-11.531938	72.787073
565.392092	-12.046239	72.792078
565.047314	4.520518	72.797082
563.995643	-4.057369	72.802087
563.403312	-4.517989	72.807092
562.837682	-3.506883	72.812097
562.277302	-7.979499	72.817102
561.228791	-12.681859	72.822106
560.450993	-3.380302	72.827111
560.300942	-9.335910	72.832116
559.419530	-9.491872	72.837121
559.115067	-14.530356	72.842126
558.222831	-1.974771	72.847130
557.626882	-3.078189	72.852135
557.328506	-14.866781	72.857140
556.175479	4.452679	72.862145
555.384662	-12.096989	72.867150
554.983824	-11.656161	72.872154
554.083572	-1.709067	72.877159
553.331057	-10.925934	72.882164
552.856625	-9.937236	72.887169
552.515186	-8.245925	72.892174
551.625694	-7.178499	72.897178
550.767480	-2.943329	72.902183
550.292324	-3.310651	72.907188
549.795769	-4.540282	72.912193
549.123809	-3.849693	72.917198
548.134342	-11.551257	72.922202
547.482070	2.475206	72.927207
547.026277	-3.786504	72.932212
545.781884	-9.876867	72.937217
545.335487	-5.708871	72.942222
545.035540	-13.840375	72.947226
544.310052	-7.215265	72.952231
544.185650	-29.812821	72.957236
543.049122	-11.897871	72.962241
542.205172	-16.863032	72.967246
541.768701	-6.758010	72.972250
540.470221	-8.492239	72.977255
540.234521	-14.090434	72.982260
539.584255	1.883181	72.987265
539.167438	-16.542639	72.992270
538.531942	-18.008747	72.997274
537.669029	-25.019276	73.002279
537.012547	-18.099243	73.007284
536.410273	-13.174736	73.012289
535.785239	-19.376363	73.017294
535.027453	-21.680823	73.022298
534.443609	-3.986359	73.027303
534.158143	-20.460392	73.032308
532.991593	-13.638872	73.037313
532.314739	-9.103016	73.042318
531.762169	-14.119319	73.047322
531.420387	-1.963638	73.052327
530.447801	-19.017323	73.057332
529.269978	-11.091753	73.062337
529.068608	-20.598241	73.067342
528.572640	-18.899658	73.072346
527.889032	-7.794936	73.077351
527.069840	-10.679375	73.082356
526.241455	-14.420181	73.087361
526.062981	-19.163347	73.092366
525.245759	-20.084857	73.097370
524.038829	-2.504017	73.102375
523.658045	-5.187065	73.107380
523.550002	-1.998604	73.112385
522.548059	-7.764889	73.117390
521.736711	-7.693887	73.122394
521.155896	-8.060140	73.127399
521.022536	-15.816065	73.132404
519.883326	-19.428510	73.137409
519.443012	-15.717205	73.142414
518.776290	-9.172413	73.147418
517.382363	-4.006676	73.152423
516.764920	-17.876397	73.157428
516.003601	-8.501769	73.162433
515.782585	-10.396585	73.167438
515.714833	-14.009406	73.172442
514.727820	0.832025	73.177447
513.956381	-11.420499	73.182452
513.406137	-12.450764	73.187457
512.777473	-11.754447	73.192462
511.670479	-8.605543	73.197466
510.961970	-6.480449	73.202471
510.822926	-8.072943	73.207476
510.106698	-13.966734	73.212481
509.318871	-11.207706	73.217486
508.677160	-5.505805	73.222490
507.971735	-3.098936	73.227495
507.643909	-13.231809	73.232500
506.503614	-11.329657	73.237505
505.849624	-19.048370	73.242510
505.470303	-17.705821	73.247514
504.064823	-7.151550	73.252519
503.647202	-8.165096	73.257524
503.001201	-2.084053	73.262529
503.092001	-14.207432	73.267534
502.383571	-7.201844	73.272538
501.125363	-16.379125	73.277543
500.551752	-17.665854	73.282548
499.855542	-8.203826	73.287553
499.716942	-7.986109	73.292558
498.968160	-7.600225	73.297562
498.088139	-12.950695	73.302567
497.586526	-14.849691	73.307572
496.402922	-10.051754	73.312577
495.785708	-8.095737	73.317582
495.224268	-6.837710	73.322586
494.646133	-8.626748	73.327591
494.796229	-16.935588	73.332596
493.734371	-9.236628	73.337601
492.981663	-11.478808	73.342606
492.464411	-17.998781	73.347610
491.270351	-14.542695	73.352615
490.871274	-12.782273	73.357620
490.218114	-11.782437	73.362625
489.510687	-13.588721	73.367630
488.742125	-22.583808	73.372634
487.974621	-20.849844	73.377639
487.833589	-28.019506	73.382644
486.776993	-12.189320	73.387649
485.913644	-18.029701	73.392654
485.762384	-10.933108	73.397658
484.564977	-13.405628	73.402663
484.539898	-24.963351	73.407668
483.055095	-7.262545	73.412673
483.052998	-14.206774	73.417678
482.467155	-12.862859	73.422682
481.435192	-15.806419	73.427687
480.542832	-19.537015	73.432692
479.906184	-6.509643	73.437697
479.944525	-16.804918	73.442702
479.171702	-21.723038	73.447706
478.102123	-9.531836	73.452711
477.756567	-8.707155	73.457716
477.156708	-13.200263	73.462721
476.246973	-13.974558	73.467726
475.513251	-7.865345	73.472730
474.923993	-3.761308	73.477735
474.891498	-22.562128	73.482740
473.227544	-11.742747	73.487745
472.770190	-11.554667	73.492750
472.160544	-15.972100	73.497754
471.345275	-3.334145	73.502759
471.017414	-18.202430	73.507764
470.110960	-9.097973	73.512769
469.761238	-17.946903	73.517774
469.229848	-13.998739	73.522778
468.156958	-6.528238	73.527783
467.415628	-19.629172	73.532788
466.531270	-9.465406	73.537793
466.287772	-1.814814	73.542798
465.903094	-5.739828	73.547802
465.091876	-13.968050	73.552807
464.790611	-32.145736	73.557812
463.744756	-17.529894	73.562817
463.278341	-17.116449	73.567822
462.393553	-17.349106	73.572826
461.529819	-16.205331	73.577831
461.323372	-17.859619	73.582836
460.501209	-5.764596	73.587841
459.537306	-14.236561	73.592846
459.184353	-19.379260	73.597850
458.418759	-19.050607	73.602855
457.704915	-23.199129	73.607860
456.445529	-12.699654	73.612865
456.415288	-20.120349	73.617870
456.175505	-23.000882	73.622874
455.250881	-18.245769	73.627879
454.572284	-22.794129	73.632884
453.673889	-12.178709	73.637889
453.386080	-27.294627	73.642894
452.470496	-22.656068	73.647898
451.727236	-14.219408	73.652903
451.400923	-22.734604	73.657908
451.019364	-21.462652	73.662913
449.963254	-33.035860	73.667918
449.024878	-16.003986	73.672922
448.531858	-10.929717	73.677927
447.401333	-25.529758	73.682932
446.363534	-26.611631	73.687937
446.326238	-27.034503	73.692942
446.231503	-22.972989	73.697946
445.689950	-24.427231	73.702951
444.759415	-24.159024	73.707956
443.697692	-20.990500	73.712961
443.154464	-22.354591	73.717966
442.894219	-29.921554	73.722970
441.762033	-19.756147	73.727975
441.170623	-14.629934	73.732980
440.674287	-14.344177	73.737985
440.284039	-15.876141	73.742990
439.044964	-21.118914	73.747994
438.323995	-11.850046	73.752999
438.053899	-20.490887	73.758004
437.493711	-14.601699	73.763009
436.791294	-12.487019	73.768014
436.282379	-14.059997	73.773018
435.138662	-10.976171	73.778023
434.637522	-19.390971	73.783028
433.620235	-9.516666	73.788033
433.306708	-22.553286	73.793038
433.119571	-21.370654	73.798042
431.737922	-8.817489	73.803047
431.007297	-18.118210	73.808052
430.345684	-13.721951	73.813057
430.123492	-12.385505	73.818062
430.073901	-22.505916	73.823066
428.771762	-17.048846	73.828071
428.226384	-16.294819	73.833076
427.523966	-9.178214	73.838081
426.414718	-12.629813	73.843086
425.547058	-23.660628	73.848090
425.224359	-15.380857	73.853095
424.959238	-16.737220	73.858100
424.272560	-11.269405	73.863105
423.169066	-19.703338	73.868110
422.444779	-22.522436	73.873114
421.874432	-8.532678	73.878119
421.835433	-14.988491	73.883124
421.010383	-6.775323	73.888129
420.380980	-17.848834	73.893134
419.783090	-24.933078	73.898138
418.692200	-19.150132	73.903143
417.788025	-10.497018	73.908148
417.305002	-8.079834	73.913153
417.070811	-18.091988	73.918158
416.175012	-19.650621	73.923162
415.120159	-9.303563	73.928167
414.933189	-15.724759	73.933172
413.918652	-19.644011	73.938177
413.647546	-18.055351	73.943182
412.876371	-19.958682	73.948186
412.071269	-19.716757	73.953191
411.567129	-25.917105	73.958196
411.071235	-5.194818	73.963201
410.492474	-16.564968	73.968206
409.968636	-21.237319	73.973210
408.651035	-19.150759	73.978215
408.239097	-22.163121	73.983220
407.327622	-17.123092	73.988225
407.221130	-12.447865	73.993230
406.552198	-20.183085	73.998234
405.570235	-14.244030	74.003239
405.270426	-27.025790	74.008244
404.163603	-19.089412	74.013249
403.045446	-24.758271	74.018254
402.546395	-12.752573	74.023258
401.984635	-16.572087	74.028263
401.953067	-14.572179	74.033268
401.315978	-7.704090	74.038273
400.795071	-13.069166	74.043278
399.789675	-18.358616	74.048282
399.146004	-8.890751	74.053287
398.078264	-18.224470	74.058292
396.858639	-16.626586	74.063297
396.604080	-17.888437	74.068302
396.611384	-13.207690	74.073306
395.779758	-4.648126	74.078311
395.225884	-19.141340	74.083316
394.584972	-2.737138	74.088321
394.189375	-15.664485	74.093326
392.953699	-16.784188	74.098330
391.938156	-16.461416	74.103335
391.733814	-23.603634	74.108340
391.060496	-12.259269	74.113345
390.570977	-25.712516	74.118350
389.435713	-23.759077	74.123354
389.175709	-19.212349	74.128359
388.897073	-25.842850	74.133364
387.430136	-11.442146	74.138369
386.865740	-24.716309	74.143374
386.308964	-22.441905	74.148378
386.001077	-15.526932	74.153383
385.190416	-23.856123	74.158388
384.116222	-8.461480	74.163393
383.533258	-19.439878	74.168398
383.408066	-12.263866	74.173402
382.535537	-8.100480	74.178407
381.965959	-22.110229	74.183412
381.182333	-9.794261	74.188417
380.467778	-15.929537	74.193422
379.835279	-26.942610	74.198426
379.044873	-10.492517	74.203431
378.590941	-10.073161	74.208436
378.070630	-18.666233	74.213441
377.038581	-9.169590	74.218446
376.330151	-17.163425	74.223450
375.493580	-9.538171	74.228455
375.295877	-24.236358	74.233460
374.456435	-9.790569	74.238465
373.902210	-8.838007	74.243470
373.643090	-14.205371	74.248474
372.739150	-16.530640	74.253479
371.870467	-20.550383	74.258484
370.616061	-11.445644	74.263489
370.356908	-25.372395	74.268494
370.325133	-18.121390	74.273498
369.353806	-8.192890	74.278503
369.151068	-15.247056	74.283508
368.392645	-5.298867	74.288513
367.192929	-23.603005	74.293518
366.551727	-7.790097	74.298522
365.704250	-4.479068	74.303527
365.416810	-14.930566	74.308532
364.586874	-6.174153	74.313537
363.445427	-9.291019	74.318542
363.170687	-10.660034	74.323546
362.620507	-5.915675	74.328551
362.668649	-20.022283	74.333556
361.392513	-14.797974	74.338561
360.584579	-17.179538	74.343566
360.516660	-17.952330	74.348570
359.483213	-15.981988	74.353575
358.763541	-11.723111	74.358580
358.045681	-1.585847	74.363585
357.105642	-17.996513	74.368590
356.581605	-22.047520	74.373594
355.675902	-12.905310	74.378599
355.625524	-14.398385	74.383604
355.112046	-9.815989	74.388609
353.978797	-19.073014	74.393614
353.528508	-8.040141	74.398618
352.675092	-10.378186	74.403623
352.206526	-22.120674	74.408628
351.143566	-9.804337	74.413633
350.588823	-9.152875	74.418638
350.411283	-18.639475	74.423642
349.282344	-18.363267	74.428647
348.331483	-24.437214	74.433652
347.930745	-13.357050	74.438657
347.598359	-11.045860	74.443662
347.301058	-12.650965	74.448666
345.870609	-4.833288	74.453671
345.578137	-10.056567	74.458676
344.945545	-5.901446	74.463681
343.942839	-10.931113	74.468686
343.448024	-19.785272	74.473690
342.471550	-9.147917	74.478695
342.295706	-16.263134	74.483700
341.952758	-7.776708	74.488705
341.052399	-28.739872	74.493710
340.207574	-15.660392	74.498714
339.790007	-15.973774	74.503719
339.083908	-14.885041	74.508724
337.955655	-11.808369	74.513729
337.311221	-5.659738	74.518734
336.853916	-13.453894	74.523738
336.179947	-15.476767	74.528743
335.442250	-23.107964	74.533748
334.833446	-13.070082	74.538753
334.165220	-9.008625	74.543758
333.823222	-11.776663	74.548762
332.641197	-7.169712	74.553767
332.204946	-14.836339	74.558772
331.700741	-18.012170	74.563777
331.243815	-17.734250	74.568782
330.610223	-18.115699	74.573786
329.305141	-7.957383	74.578791
329.173259	-18.879924	74.583796
328.361951	-9.695980	74.588801
327.217579	-10.368171	74.593806
327.342751	-19.346366	74.598810
326.536965	-7.435271	74.603815
325.497143	-20.020230	74.608820
324.948327	-18.338417	74.613825
324.244872	-12.519413	74.618830
324.100059	-1.380684	74.623834
323.054251	-12.252183	74.628839
322.571452	-18.268261	74.633844
321.892040	-18.088915	74.638849
320.748090	-18.086258	74.643854
320.034028	-15.856155	74.648858
319.404065	-13.038658	74.653863
319.244933	-15.889453	74.658868
318.644018	-17.693737	74.663873
317.637281	-16.312664	74.668878
316.749365	-14.028044	74.673882
316.128679	-9.244057	74.678887
315.924175	-17.188879	74.683892
315.423186	-14.065520	74.688897
314.503982	-16.044570	74.693902
314.211724	-7.946255	74.698906
312.987326	-16.411321	74.703911
312.241781	-14.414310	74.708916
311.535854	-12.133463	74.713921
311.459356	-14.637895	74.718926
311.007214	-20.270938	74.723930
309.605222	-21.750430	74.728935
309.529670	-23.225298	74.733940
308.488369	-14.905103	74.738945
307.421190	-12.899403	74.743950
306.661518	-21.449571	74.748954
306.141119	-11.017358	74.753959
305.937865	-17.139485	74.758964
305.479644	-22.148684	74.763969
304.811244	-17.599935	74.768974
304.002343	-11.839810	74.773978
303.004782	-10.655729	74.778983
302.626160	-15.650808	74.783988
301.635882	-8.258070	74.788993
300.874810	-10.943539	74.793998
300.765067	-20.906119	74.799002
300.277165	-16.605325	74.804007
299.489099	-20.220012	74.809012
298.689484	-11.250807	74.814017
298.032145	-13.564892	74.819022
297.030048	-12.824770	74.824026
296.076524	-16.755270	74.829031
295.826323	-13.250849	74.834036
295.746548	-10.776497	74.839041
294.693549	-16.564494	74.844046
293.976470	-19.394161	74.849050
293.041852	2.207008	74.854055
292.725034	-13.940275	74.859060
291.818537	-7.860249	74.864065
291.046306	-13.240428	74.869070
290.542287	-21.381923	74.874074
290.177179	-12.343206	74.879079
289.518172	-15.757696	74.884084
288.715322	-10.410101	74.889089
288.089181	-14.389627	74.894094
287.858422	-10.788959	74.899098
286.689401	-10.498449	74.904103
286.098282	-7.232989	74.909108
285.910870	-11.470096	74.914113
284.653855	-15.643943	74.919118
284.152326	-20.136897	74.924122
283.300106	-11.304378	74.929127
283.091543	-11.789831	74.934132
281.688670	-15.177210	74.939137
281.206169	-4.188079	74.944142
280.680555	-9.082459	74.949146
280.019002	-9.796894	74.954151
279.599159	-22.370264	74.959156
278.757411	-7.212908	74.964161
278.143359	0.093066	74.969166
277.654305	-15.881682	74.974170
276.367476	0.628643	74.979175
275.940263	-8.141665	74.984180
275.398327	-9.190545	74.989185
275.027779	-4.151540	74.994190
274.590323	-3.548718	74.999194
273.300122	-11.413515	75.004199
273.106332	-10.881071	75.009204
271.828187	-9.921901	75.014209
271.020549	-11.921872	75.019214
270.796673	-12.553111	75.024218
269.845029	-9.201797	75.029223
269.992673	-15.395622	75.034228
268.858107	-19.087524	75.039233
267.962878	-18.760226	75.044238
267.564239	-11.728281	75.049242
266.795356	-17.044331	75.054247
266.746537	-19.616247	75.059252
265.272800	-19.945758	75.064257
264.478796	-16.706301	75.069262
264.552715	-21.929618	75.074266
263.702568	-17.277775	75.079271
263.150937	-19.555084	75.084276
262.784524	-9.656749	75.089281
261.395577	-12.901262	75.094286
260.583959	-24.768801	75.099290
259.674063	-8.285450	75.104295
259.425483	-7.134011	75.109300
259.062146	-0.650140	75.114305
258.924832	-24.144390	75.119310
257.772336	-14.057677	75.124314
256.618486	-9.286458	75.129319
256.660023	-17.122262	75.134324
255.664738	5.757989	75.139329
254.785381	-20.289245	75.144334
254.366999	5.644949	75.149338
253.698248	-9.798121	75.154343
252.854204	-21.668375	75.159348
252.007477	-1.172426	75.164353
251.822404	-12.570586	75.169358
251.217930	-15.897566	75.174362
250.009638	0.098795	75.179367
249.890409	-15.105448	75.184372
249.088054	-7.685881	75.189377
248.648574	-6.344744	75.194382
247.884418	-23.576558	75.199386
246.968326	-19.716838	75.204391
246.462271	-17.135111	75.209396
246.241007	-19.200161	75.214401
245.269225	-7.210551	75.219406
244.946720	-20.712451	75.224410
243.437046	-8.045760	75.229415
242.585032	-1.589640	75.234420
242.227533	-7.573637	75.239425
241.904867	-13.438610	75.244430
241.504391	-18.266195	75.249434
240.146016	-12.139351	75.254439
240.090127	-22.433768	75.259444
239.156607	-5.617074	75.264449
238.555587	-10.400077	75.269454
237.845307	-9.537722	75.274458
236.844049	-1.996558	75.279463
236.562635	-8.844206	75.284468
236.235179	-12.350956	75.289473
235.080035	-4.104043	75.294478
234.567288	-3.613786	75.299482
234.018005	-14.182779	75.304487
233.180130	-9.378345	75.309492
232.197305	-6.343732	75.314497
231.906247	-12.092321	75.319502
231.397985	-7.308893	75.324506
230.500581	2.847558	75.329511
229.994007	-7.218910	75.334516
229.490285	-12.993518	75.339521
228.503850	-10.595395	75.344526
227.585009	-12.207053	75.349530
226.709635	-8.331737	75.354535
226.572564	-13.688573	75.359540
226.147548	-12.010706	75.364545
225.801557	-11.993293	75.369550
224.722275	-21.386575	75.374554
223.902087	-0.245172	75.379559
223.656072	-15.176895	75.384564
222.672385	-11.959223	75.389569
221.910344	-8.795807	75.394574
221.388961	-17.279855	75.399578
220.891821	-14.529240	75.404583
219.585965	-15.093638	75.409588
219.041709	-6.127275	75.414593
218.262506	-10.135995	75.419598
218.130766	-16.176474	75.424602
217.239722	-13.060298	75.429607
216.265056	-6.218779	75.434612
215.899861	-12.729802	75.439617
215.427214	-15.082767	75.444622
215.196245	-22.040945	75.449626
213.940702	-10.204780	75.454631
213.617916	-14.552755	75.459636
213.084444	-8.360292	75.464641
212.156263	-9.185161	75.469646
211.514171	-17.959034	75.474650
210.861113	-2.733975	75.479655
210.126493	-13.959363	75.484660
209.112287	-7.389073	75.489665
208.439036	-10.741345	75.494670
208.035819	-16.178745	75.499674
207.529362	-18.911080	75.504679
207.057881	-27.902949	75.509684
205.929706	-22.011481	75.514689
205.559289	-18.107858	75.519694
204.925156	-26.592843	75.524698
203.700696	-5.137845	75.529703
203.424671	-21.271096	75.534708
203.195405	-27.087870	75.539713
202.440378	-14.705473	75.544718
201.329265	-13.700361	75.549722
200.526058	0.375431	75.554727
200.368587	-19.528157	75.559732
199.790547	-7.211815	75.564737
198.527862	-17.536175	75.569742
198.473994	-11.186794	75.574746
197.541478	-18.813686	75.579751
196.565594	-18.516080	75.584756
195.691276	-14.699270	75.589761
195.345652	-7.738844	75.594766
195.169190	-24.679564	75.599770
194.423261	-12.487841	75.604775
193.309203	-11.837056	75.609780
192.774029	-14.008167	75.614785
191.854443	-7.965446	75.619790
191.958445	-7.184017	75.624794
191.199999	-6.739731	75.629799
190.261770	-8.091250	75.634804
189.720469	-7.109171	75.639809
189.115929	-9.903134	75.644814
188.312937	-15.715169	75.649818
187.520582	-17.963541	75.654823
187.204928	-7.196541	75.659828
186.257954	-11.240000	75.664833
185.492561	-14.974951	75.669838
185.308376	-20.193385	75.674842
184.443116	-10.314859	75.679847
183.730624	-20.414702	75.684852
182.707034	-21.451420	75.689857
182.173238	-10.890908	75.694862
182.052030	-18.077886	75.699866
180.666381	-15.195066	75.704871
180.181241	-16.867967	75.709876
179.498045	-13.534192	75.714881
179.026821	-21.532654	75.719886
178.761982	-18.875838	75.724890
177.515759	-16.950344	75.729895
177.254131	-22.842378	75.734900
176.408705	-9.740688	75.739905
175.707261	-16.843039	75.744910
174.882635	-24.176472	75.749914
174.042922	-9.872524	75.754919
174.175750	-20.821472	75.759924
173.268471	-9.870263	75.764929
172.408606	-6.817387	75.769934
171.842389	-13.461923	75.774938
170.962470	-16.893191	75.779943
170.614746	-14.029201	75.784948
169.811820	-18.540301	75.789953
168.854883	-12.215663	75.794958
168.796975	-25.545267	75.799962
167.788010	-9.224293	75.804967
167.260166	-21.116537	75.809972
166.573026	-14.163160	75.814977
165.798604	-12.650340	75.819982
164.844848	-17.246195	75.824986
164.332902	-17.555537	75.829991
163.876448	-17.115241	75.834996
163.157884	-15.387407	75.840001
162.586654	-19.292074	75.845006
161.904460	-17.338236	75.850010
161.307779	-19.551568	75.855015
160.848488	-22.173145	75.860020
159.723837	-2.583740	75.865025
158.768746	-11.236732	75.870030
158.744198	-17.328986	75.875034
158.166805	1.655947	75.880039
157.523896	-17.769699	75.885044
156.548692	-6.988996	75.890049
156.095394	-11.289344	75.895054
155.615387	-15.686354	75.900058
154.060780	-5.923399	75.905063
153.594968	-18.293869	75.910068
153.118851	-10.131543	75.915073
152.743777	-8.781737	75.920078
152.053441	-17.770238	75.925082
151.119159	-6.239150	75.930087
150.711587	-14.645134	75.935092
150.406844	-26.424713	75.940097
149.229247	-6.379031	75.945102
148.668566	-13.882272	75.950106
148.165606	-11.731513	75.955111
147.124918	-9.797777	75.960116
146.418596	-8.040352	75.965121
145.846754	-5.990567	75.970126
145.612534	-15.209484	75.975130
144.844802	-7.666107	75.980135
144.327796	-16.169752	75.985140
143.365987	-3.412179	75.990145
142.660226	-3.703227	75.995150
141.666080	-21.825531	76.000154
141.289515	-18.166916	76.005159
141.117510	-22.078465	76.010164
140.116139	-13.256821	76.015169
139.316566	-9.045071	76.020174
138.617506	-16.997734	76.025178
137.844044	-4.399498	76.030183
137.545914	-17.548878	76.035188
137.114056	-17.361648	76.040193
135.915811	-11.328093	76.045198
135.421632	-26.095635	76.050202
134.707346	-6.030790	76.055207
134.086251	-11.625814	76.060212
133.000963	-30.440017	76.065217
132.544188	-14.599736	76.070222
132.206481	-5.866564	76.075226
131.840028	-13.801302	76.080231
131.049849	-21.286861	76.085236
130.344275	-24.219230	76.090241
129.796649	-7.136055	76.095246
129.037050	-10.547072	76.100250
128.115962	-6.472054	76.105255
127.444519	-27.909968	76.110260
127.124865	-23.159758	76.115265
126.077397	-5.783998	76.120270
125.327881	-18.295293	76.125274
124.825377	-8.097718	76.130279
124.471899	-11.079924	76.135284
123.515568	-6.403220	76.140289
122.699804	-10.688338	76.145294
122.790298	-20.247597	76.150298
121.394436	1.513874	76.155303
120.634410	-7.320011	76.160308
120.623095	-5.182991	76.165313
120.102816	-17.183657	76.170318
118.924507	-11.627918	76.175322
118.039138	-8.722341	76.180327
117.699929	-9.947009	76.185332
116.759217	-9.199257	76.190337
115.889696	-8.161670	76.195342
115.676733	-12.637523	76.200346
115.038350	-6.649081	76.205351
114.668630	-8.330912	76.210356
113.566334	-8.501952	76.215361
112.641691	-5.020850	76.220366
112.706857	-16.766377	76.225370
111.555148	-12.090053	76.230375
110.726856	-9.568875	76.235380
110.545185	-11.059928	76.240385
109.743351	-11.751946	76.245390
109.372530	-9.284796	76.250394
107.920107	-8.520093	76.255399
107.523829	-15.398281	76.260404
107.377120	-13.331131	76.265409
106.324802	-17.862359	76.270414
105.832408	-24.102342	76.275418
105.269221	-16.467004	76.280423
104.451974	-22.019697	76.285428
103.386689	-19.156386	76.290433
102.950977	-9.272224	76.295438
102.622960	-23.708299	76.300442
101.845759	-13.727107	76.305447
101.190583	-10.454548	76.310452
100.230331	-16.783921	76.315457
99.615057	-8.832778	76.320462
99.225315	-13.288321	76.325466
98.330780	-24.554381	76.330471
97.737427	-19.085611	76.335476
97.248715	-5.052075	76.340481
96.635730	-21.435900	76.345486
95.855034	-17.164075	76.350490
94.857161	-9.437336	76.355495
94.503195	-21.387243	76.360500
94.016010	0.180444	76.365505
93.209380	-15.207447	76.370510
92.423340	-28.610145	76.375514
91.834045	-10.820189	76.380519
91.296575	-12.571456	76.385524
90.288499	-20.049058	76.390529
89.494584	-1.835391	76.395534
89.359700	-26.254031	76.400538
88.646734	-16.417117	76.405543
87.940684	-5.996273	76.410548
87.369524	-20.567030	76.415553
86.403365	-11.648486	76.420558
86.181739	-20.126680	76.425562
84.927419	-19.346250	76.430567
84.572011	-5.725042	76.435572
83.998811	-14.725891	76.440577
83.247019	-18.503973	76.445582
82.891504	-13.315969	76.450586
81.725032	-7.989174	76.455591
81.066704	-19.445857	76.460596
80.605300	-14.753456	76.465601
79.677351	-9.597158	76.470606
79.399516	-21.347899	76.475610
78.809554	-2.458733	76.480615
78.269732	-20.222962	76.485620
77.378507	-30.142870	76.490625
76.225368	-5.630584	76.495630
76.057022	-10.039434	76.500634
75.712110	-6.144592	76.505639
74.485080	-14.620136	76.510644
73.760759	-15.712419	76.515649
73.290660	-10.091417	76.520654
73.080952	-23.078265	76.525658
72.008298	-11.121409	76.530663
70.977846	-21.325032	76.535668
70.776664	-15.283313	76.540673
70.297213	-8.990639	76.545678
69.523599	-15.212574	76.550682
68.469371	-4.103863	76.555687
68.288649	-15.543677	76.560692
67.971792	-13.585003	76.565697
66.556082	-3.872537	76.570702
66.291084	-21.516592	76.575706
65.534412	-21.433659	76.580711
64.462613	-20.505716	76.585716
63.663924	-8.337091	76.590721
63.027637	-8.828424	76.595726
62.985199	-19.719452	76.600730
62.374085	-14.123267	76.605735
61.776962	-14.980376	76.610740
61.086930	-8.956880	76.615745
60.165669	-12.498201	76.620750
59.687563	-6.954763	76.625754
58.504786	-11.007866	76.630759
57.747404	-8.551595	76.635764
57.704660	-11.605423	76.640769
56.880313	-7.176819	76.645774
55.715759	-11.778431	76.650778
54.991695	-15.559349	76.655783
54.907487	-13.519511	76.660788
54.612341	-19.841401	76.665793
53.777497	-10.533798	76.670798
53.044895	-18.559923	76.675802
52.263351	-8.926518	76.680807
51.550698	-10.315534	76.685812
50.621871	-20.713544	76.690817
50.142996	-6.583809	76.695822
49.922659	-18.148181	76.700826
48.954811	7.257061	76.705831
48.448091	-13.797113	76.710836
47.631557	-8.835186	76.715841
47.012569	-15.766144	76.720846
46.254320	-21.722446	76.725850
45.117145	-5.021460	76.730855
44.699647	-7.706448	76.735860
44.321341	-15.729156	76.740865
43.835753	-14.730702	76.745870
43.378422	-20.924224	76.750874
42.371539	-5.084501	76.755879
41.523378	-16.012596	76.760884
40.802015	-20.082510	76.765889
39.885849	-16.386705	76.770894
39.583400	-12.820320	76.775898
39.142473	-18.052978	76.780903
38.788049	-20.478373	76.785908
37.571986	6.540194	76.790913
36.879733	-19.495741	76.795918
36.464715	-7.476610	76.800922
36.053360	-10.829601	76.805927
35.186043	-16.006867	76.810932
34.531363	-9.296748	76.815937
33.656570	7.922204	76.820942
32.992261	-26.034178	76.825946
31.970124	-15.208116	76.830951
32.125374	-9.983304	76.835956
31.392492	-21.082736	76.840961
30.090594	-5.140764	76.845966
29.740821	-15.803006	76.850970
29.344589	-10.108628	76.855975
28.712064	-12.361938	76.860980
27.680685	-10.815976	76.865985
26.994664	-6.915608	76.870990
26.758572	-17.878243	76.875994
25.330214	-15.346482	76.880999
24.687653	-19.556688	76.886004
24.374717	-11.100267	76.891009
23.513869	-9.996226	76.896014
23.670719	-15.806755	76.901018
22.648157	-12.824073	76.906023
21.600671	-18.729503	76.911028
21.354311	-15.348675	76.916033
20.878808	-8.624557	76.921038
20.132740	-4.561650	76.926042
19.041972	-7.487738	76.931047
18.805776	-13.358574	76.936052
17.892599	-15.188663	76.941057
17.080420	-5.485709	76.946062
16.192498	-1.354444	76.951066
16.193054	-14.734356	76.956071
15.025404	-14.093865	76.961076
14.586080	-13.033402	76.966081
13.744512	-20.168533	76.971086
13.401686	-14.274523	76.976090
12.422337	-9.108428	76.981095
11.965941	-10.410578	76.986100
11.247555	-12.602881	76.991105
10.694989	-14.309144	76.996110
10.050333	-15.235925	77.001114
8.829644	-22.559730	77.006119
8.578104	-28.484878	77.011124
8.267576	-16.250617	77.016129
7.376475	-5.984738	77.021134
6.761057	-26.628891	77.026139
5.795392	-8.968122	77.031143
5.547323	-11.547667	77.036148
4.787948	-12.974946	77.041153
3.843898	-5.942708	77.046158