Mon Mar 08 18:22:01 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.400188	95.418620	0.000000
-1.005849	82.166918	0.005005
-1.674588	50.322721	0.010010
-3.844203	9.201499	0.015014
-8.586292	3.915385	0.020019
-14.033187	12.354947	0.025024
-18.992361	7.589160	0.030029
-23.093893	5.933380	0.035034
-26.933803	5.744950	0.040038
-30.383627	11.177389	0.045043
-34.248827	7.903889	0.050048
-37.834244	-5.518899	0.055053
-41.569017	1.329318	0.060058
-45.352082	12.785017	0.065062
-48.928165	9.000239	0.070067
-53.193319	14.938077	0.075072
-56.687523	13.809911	0.080077
-60.037650	16.624629	0.085082
-63.956564	13.858041	0.090086
-67.538015	6.710655	0.095091
-71.664393	9.431618	0.100096
-75.262306	1.782270	0.105101
-79.440308	4.571403	0.110106
-83.000420	9.904819	0.115110
-86.602684	1.961306	0.120115
-90.509205	13.525073	0.125120
-93.987677	17.066757	0.130125
-97.837811	4.865800	0.135130
-101.702571	7.639685	0.140134
-105.279772	4.214701	0.145139
-109.320677	10.488997	0.150144
-113.268436	8.291618	0.155149
-116.392250	7.709966	0.160154
-120.386451	14.880382	0.165158
-124.233949	-0.127796	0.170163
-128.269266	7.157995	0.175168
-132.273401	-1.954442	0.180173
-135.742424	-6.131464	0.185178
-139.936643	13.134038	0.190182
-143.253188	-2.255281	0.195187
-147.301084	13.946660	0.200192
-150.689543	8.479525	0.205197
-154.618177	9.864991	0.210202
-158.835681	11.381712	0.215206
-162.215480	9.189972	0.220211
-165.873365	15.288128	0.225216
-169.217478	8.345866	0.230221
-173.009816	5.135080	0.235226
-176.905511	18.934846	0.240230
-180.279374	4.784692	0.245235
-184.601788	15.735334	0.250240
-188.605968	11.780976	0.255245
-192.088923	6.478786	0.260250
-195.689175	17.238509	0.265254
-199.413852	8.294464	0.270259
-203.463702	19.073914	0.275264
-207.336607	15.661583	0.280269
-211.022761	15.040495	0.285274
-214.945771	18.028850	0.290278
-218.058233	11.308296	0.295283
-222.025480	8.111312	0.300288
-225.842855	14.542500	0.305293
-229.840492	14.862092	0.310298
-234.127634	21.437655	0.315302
-237.366550	14.628503	0.320307
-241.039320	12.182451	0.325312
-244.652185	7.350486	0.330317
-248.307086	10.001224	0.335322
-252.202369	11.897165	0.340326
-255.588338	1.916759	0.345331
-260.423908	16.194652	0.350336
-263.722700	4.320700	0.355341
-267.403111	12.136665	0.360346
-270.897021	-0.302188	0.365350
-274.275826	6.558936	0.370355
-278.564506	4.222295	0.375360
-282.457029	6.993011	0.380365
-285.920004	13.224223	0.385370
-290.344726	11.816023	0.390374
-293.449282	10.570814	0.395379
-297.516283	7.697372	0.400384
-301.449534	8.131379	0.405389
-304.892905	8.700068	0.410394
-308.749886	7.811524	0.415398
-312.251370	9.774001	0.420403
-316.656863	11.216931	0.425408
-320.262410	13.202340	0.430413
-323.687095	16.835103	0.435418
-327.530475	5.986428	0.440422
-330.957798	13.910309	0.445427
-335.045073	5.590476	0.450432
-338.882669	9.757512	0.455437
-342.547323	7.963151	0.460442
-346.604515	4.818582	0.465446
-349.864286	14.302077	0.470451
-353.939561	11.972499	0.475456
-357.476545	10.820067	0.480461
-361.457054	2.382318	0.485466
-365.642091	11.445881	0.490470
-369.147423	5.668160	0.495475
-372.594886	11.507525	0.500480
-376.303846	6.077703	0.505485
-380.363332	-1.768686	0.510490
-384.218062	9.598021	0.515494
-387.393469	7.752420	0.520499
-391.604883	17.668601	0.525504
-395.282425	-1.488193	0.530509
-398.948140	0.760815	0.535514
-402.920862	8.174239	0.540518
-406.657528	5.666113	0.545523
-410.592516	11.335806	0.550528
-414.155499	10.332683	0.555533
-417.600480	6.896523	0.560538
-421.630685	12.953582	0.565542
-424.900136	9.390060	0.570547
-429.006343	9.814048	0.575552
-432.935169	14.527207	0.580557
-436.703523	0.180270	0.585562
-440.628588	6.892317	0.590566
-444.310068	10.520525	0.595571
-447.910529	7.774681	0.600576
-451.749860	1.323487	0.605581
-455.433653	7.716343	0.610586
-459.703316	15.074784	0.615590
-462.785702	2.335560	0.620595
-466.631565	5.234730	0.625600
-470.501611	11.925424	0.630605
-473.961444	3.932972	0.635610
-478.100105	11.879194	0.640614
-481.499586	-0.405677	0.645619
-485.436273	12.538532	0.650624
-489.616361	11.659309	0.655629
-493.253791	-5.296087	0.660634
-497.015379	9.490344	0.665638
-500.715479	2.206481	0.670643
-504.757112	6.302288	0.675648
-508.137957	14.546974	0.680653
-511.507924	6.444035	0.685658
-514.980461	14.492074	0.690662
-519.059856	5.567371	0.695667
-523.324347	9.525350	0.700672
-527.088107	3.264051	0.705677
-530.535302	15.125677	0.710682
-534.588941	20.500724	0.715686
-538.326203	3.935060	0.720691
-541.939455	9.909944	0.725696
-545.692685	10.530050	0.730701
-549.626699	2.856297	0.735706
-553.491948	13.412850	0.740710
-557.021276	6.559091	0.745715
-560.937325	8.864102	0.750720
-564.610823	3.195543	0.755725
-568.171937	7.080663	0.760730
-572.506888	12.726201	0.765734
-575.531306	7.952131	0.770739
-579.556679	14.216823	0.775744
-583.274190	6.391852	0.780749
-587.058268	3.046384	0.785754
-591.205120	11.840882	0.790758
-594.782898	5.438025	0.795763
-598.646869	10.021244	0.800768
-602.279844	4.477152	0.805773
-605.475057	1.739347	0.810778
-609.569028	10.738305	0.815782
-613.168361	3.567830	0.820787
-617.425841	5.332999	0.825792
-621.024063	-0.740135	0.830797
-624.589612	3.699256	0.835802
-628.750063	-0.480097	0.840806
-632.207434	6.521786	0.845811
-636.237840	20.682780	0.850816
-639.681741	17.355580	0.855821
-643.347056	6.400159	0.860826
-647.254968	5.282196	0.865830
-650.968396	1.599132	0.870835
-654.907380	-3.383495	0.875840
-658.611704	-8.307419	0.880845
-662.485395	5.388614	0.885850
-666.522486	0.596714	0.890854
-669.925184	5.699244	0.895859
-673.703995	9.272390	0.900864
-677.468893	-1.958776	0.905869
-681.146416	-7.415198	0.910874
-685.034841	0.338418	0.915878
-688.310803	9.541088	0.920883
-692.654594	6.695217	0.925888
-695.965660	-3.878345	0.930893
-699.575221	-5.269387	0.935898
-703.796885	0.337776	0.940902
-707.601991	-2.333963	0.945907
-711.024525	-7.018996	0.950912
-715.300556	-1.477239	0.955917
-718.777789	5.002839	0.960922
-722.778097	8.234587	0.965926
-726.200121	-0.263383	0.970931
-730.307122	-2.254513	0.975936
-733.612805	0.039962	0.980941
-737.150495	1.234596	0.985946
-741.131172	1.233805	0.990950
-745.236813	1.577828	0.995955
-749.019759	2.611414	1.000960
-752.818043	0.205150	1.005965
-756.188284	-3.750200	1.010970
-760.206584	10.226125	1.015974
-763.910340	-0.655139	1.020979
-768.025578	4.367453	1.025984
-771.601378	3.748522	1.030989
-775.072855	1.408326	1.035994
-779.037350	7.982137	1.040998
-782.654432	2.054192	1.046003
-786.786422	6.538628	1.051008
-790.415804	4.942746	1.056013
-793.940171	5.438359	1.061018
-797.955972	11.343926	1.066022
-801.404728	4.955465	1.071027
-805.311565	9.596322	1.076032
-809.141268	6.122900	1.081037
-812.711003	6.617908	1.086042
-816.613013	16.674563	1.091046
-820.009193	0.928465	1.096051
-824.088512	15.285211	1.101056
-827.744268	1.605320	1.106061
-831.554634	1.579034	1.111066
-835.551386	13.364917	1.116070
-839.062660	4.471401	1.121075
-842.632981	3.477984	1.126080
-846.580034	3.910366	1.131085
-850.467283	-3.153777	1.136090
-854.385327	1.257149	1.141094
-857.910532	2.073096	1.146099
-861.698887	9.099827	1.151104
-865.609166	5.934255	1.156109
-869.112233	-1.929250	1.161114
-873.414119	17.964851	1.166118
-876.929341	10.559011	1.171123
-880.550051	3.412882	1.176128
-884.210223	0.133244	1.181133
-887.624001	7.726145	1.186138
-891.889899	4.527592	1.191142
-895.481819	-6.574741	1.196147
-899.196879	-2.831674	1.201152
-903.207891	9.428076	1.206157
-907.025098	3.724704	1.211162
-910.764300	3.119496	1.216166
-914.460984	5.301706	1.221171
-918.484454	-0.611503	1.226176
-921.996523	9.838677	1.231181
-925.214837	-7.821614	1.236186
-929.353175	7.268509	1.241190
-932.686127	-8.249399	1.246195
-936.777649	-1.566721	1.251200
-940.718504	-4.829770	1.256205
-944.434860	1.684129	1.261210
-948.433719	11.119417	1.266214
-951.909993	-30.180935	1.271219
-955.814712	8.788178	1.276224
-959.734133	-6.549180	1.281229
-963.427442	-8.514592	1.286234
-967.314025	4.732974	1.291238
-970.703824	-4.749000	1.296243
-974.532726	-0.583934	1.301248
-978.322248	-2.303715	1.306253
-981.879127	-4.267262	1.311258
-985.967644	1.508321	1.316262
-989.633766	-17.332274	1.321267
-993.493784	17.801135	1.326272
-997.358369	-5.744632	1.331277
-1000.600463	-11.227594	1.336282
-1004.648014	1.613707	1.341286
-1008.268222	-4.355948	1.346291
-1012.110575	-2.429395	1.351296
-1016.241902	1.501846	1.356301
-1019.751097	-11.401672	1.361306
-1023.347018	-1.138211	1.366310
-1027.525905	9.655293	1.371315
-1030.956460	8.382782	1.376320
-1034.781503	-0.250512	1.381325
-1038.375066	-17.260847	1.386330
-1042.246466	0.853754	1.391334
-1045.821421	8.332311	1.396339
-1049.625041	-0.411610	1.401344
-1053.913661	-3.439077	1.406349
-1057.332422	-2.002805	1.411354
-1061.446267	8.141721	1.416358
-1064.733347	-2.141818	1.421363
-1068.477773	-2.307568	1.426368
-1072.509134	6.371489	1.431373
-1076.120238	1.762896	1.436378
-1079.689122	-2.139700	1.441382
-1083.496109	-10.302731	1.446387
-1087.409740	-0.336843	1.451392
-1091.138028	5.289838	1.456397
-1094.948109	-8.607735	1.461402
-1099.123639	-1.709508	1.466406
-1102.569634	-8.249318	1.471411
-1106.195074	-12.939137	1.476416
-1110.047525	-14.271763	1.481421
-1113.254381	-6.643856	1.486426
-1117.433273	1.410783	1.491430
-1121.047588	-12.177455	1.496435
-1125.037633	-12.418930	1.501440
-1129.023665	-3.944146	1.506445
-1132.600995	-12.221098	1.511450
-1136.434924	5.857691	1.516454
-1140.151721	-12.220794	1.521459
-1143.853323	-4.486887	1.526464
-1147.309796	-5.439705	1.531469
-1150.702443	-0.757561	1.536474
-1155.109011	7.445528	1.541478
-1159.021817	2.533698	1.546483
-1162.916593	-0.315319	1.551488
-1166.371830	-9.635135	1.556493
-1170.232095	-14.549039	1.561498
-1173.988917	8.874069	1.566502
-1177.850767	1.853737	1.571507
-1181.302811	-1.944398	1.576512
-1185.138729	-2.907405	1.581517
-1188.705226	-4.471724	1.586522
-1192.922388	4.595206	1.591526
-1196.869606	1.335193	1.596531
-1200.247760	1.915247	1.601536
-1204.217348	4.933162	1.606541
-1207.801061	1.100945	1.611546
-1211.393092	11.244219	1.616550
-1214.848351	-5.721726	1.621555
-1218.879820	5.431682	1.626560
-1222.964833	16.445448	1.631565
-1226.400331	4.072906	1.636570
-1230.200596	8.344181	1.641574
-1234.017440	6.302782	1.646579
-1238.134080	3.989262	1.651584
-1241.928598	12.256982	1.656589
-1245.234421	8.437119	1.661594
-1249.238870	16.615453	1.666598
-1252.867521	5.046526	1.671603
-1256.500988	-1.494583	1.676608
-1260.383914	6.653278	1.681613
-1263.969027	12.266776	1.686618
-1267.833846	12.781319	1.691622
-1271.697127	6.286473	1.696627
-1275.582087	8.513571	1.701632
-1279.607782	2.971928	1.706637
-1283.020619	1.186055	1.711642
-1286.743533	12.419497	1.716646
-1290.072427	4.054148	1.721651
-1294.096760	5.669685	1.726656
-1298.076480	12.797103	1.731661
-1301.833345	4.464003	1.736666
-1306.088199	2.349337	1.741670
-1309.583232	5.923794	1.746675
-1312.991598	18.059357	1.751680
-1316.693357	10.753456	1.756685
-1320.221297	8.754262	1.761690
-1324.453811	7.768240	1.766694
-1328.014935	11.433723	1.771699
-1331.852052	9.455654	1.776704
-1335.789162	3.669710	1.781709
-1339.111609	5.765873	1.786714
-1342.992137	6.918531	1.791718
-1346.681006	2.098908	1.796723
-1350.731154	-6.605021	1.801728
-1354.883077	7.921870	1.806733
-1358.380132	0.863957	1.811738
-1362.132094	14.607792	1.816742
-1365.937942	9.368557	1.821747
-1369.606499	3.960705	1.826752
-1373.438160	16.323374	1.831757
-1376.864085	10.370516	1.836762
-1380.782733	15.223924	1.841766
-1384.529931	5.780884	1.846771
-1388.111146	18.231208	1.851776
-1392.348204	15.519376	1.856781
-1395.517770	8.055873	1.861786
-1399.577111	8.431478	1.866790
-1403.357646	9.088863	1.871795
-1406.873383	19.071985	1.876800
-1410.947091	16.288305	1.881805
-1414.222658	6.268366	1.886810
-1418.464835	11.463776	1.891814
-1422.095197	0.330628	1.896819
-1425.996649	3.161399	1.901824
-1429.875414	13.076525	1.906829
-1433.490144	17.613293	1.911834
-1437.253187	10.339485	1.916838
-1441.061999	14.330209	1.921843
-1444.511002	1.294752	1.926848
-1448.798837	17.783103	1.931853
-1452.521044	13.670692	1.936858
-1456.080168	8.994466	1.941862
-1459.669750	8.148582	1.946867
-1463.541548	13.970699	1.951872
-1467.144278	1.827167	1.956877
-1470.846583	9.662608	1.961882
-1474.730086	14.338665	1.966886
-1478.458222	3.416799	1.971891
-1482.288483	10.296672	1.976896
-1486.079696	15.216574	1.981901
-1489.868265	13.883816	1.986906
-1493.931357	19.815461	1.991910
-1497.582598	9.739120	1.996915
-1501.519483	10.094496	2.006912
-1502.184181	7.065472	2.016909
-1499.887069	15.687911	2.026906
-1496.676818	14.700334	2.036902
-1494.748756	6.847879	2.046899
-1493.011044	11.694817	2.056896
-1491.187664	17.977448	2.066893
-1489.086702	20.404221	2.076890
-1487.302513	10.836464	2.086886
-1485.394874	13.497872	2.096883
-1483.326110	15.050371	2.106880
-1481.393764	19.247232	2.116877
-1479.499222	15.164198	2.126874
-1477.506442	11.715933	2.136870
-1475.951817	11.254019	2.146867
-1474.372577	13.622249	2.156864
-1472.218656	12.788068	2.166861
-1470.096253	11.166340	2.176858
-1467.962121	7.624400	2.186854
-1466.402649	12.154126	2.196851
-1464.371110	4.979832	2.206848
-1462.621013	9.940068	2.216845
-1460.742587	5.196503	2.226842
-1458.856816	6.378869	2.236838
-1456.978042	4.838793	2.246835
-1454.762593	6.026791	2.256832
-1453.098241	1.366457	2.266829
-1451.622993	8.628504	2.276826
-1449.489673	1.941588	2.286822
-1447.559239	0.121682	2.296819
-1445.700177	9.267455	2.306816
-1443.568021	4.499065	2.316813
-1441.993206	11.772020	2.326810
-1439.999054	-1.340740	2.336806
-1438.015454	-0.848202	2.346803
-1436.231468	1.949881	2.356800
-1434.532817	1.607033	2.366797
-1432.352514	-0.464437	2.376794
-1430.535756	-2.226656	2.386790
-1428.745574	-0.144790	2.396787
-1427.132780	4.565890	2.406784
-1424.888106	-7.325442	2.416781
-1422.845404	2.441441	2.426778
-1421.019042	-12.444350	2.436774
-1419.311673	1.062900	2.446771
-1417.283735	-3.125119	2.456768
-1415.473274	-2.303275	2.466765
-1413.643643	-6.175343	2.476762
-1411.774308	-8.170165	2.486758
-1409.888527	2.644967	2.496755
-1408.188657	4.652892	2.506752
-1406.143438	0.087921	2.516749
-1404.300462	-4.343620	2.526746
-1402.137575	2.549433	2.536742
-1400.761773	3.376143	2.546739
-1398.794083	-5.106234	2.556736
-1396.680579	5.028272	2.566733
-1394.777499	-0.290741	2.576730
-1392.765979	-0.874692	2.586726
-1391.013400	1.871616	2.596723
-1389.563063	0.592809	2.606720
-1387.223273	-2.400955	2.616717
-1385.276846	-1.441389	2.626714
-1384.034037	4.206411	2.636710
-1381.664388	1.117876	2.646707
-1379.783562	5.550430	2.656704
-1377.902932	7.892583	2.666701
-1376.138892	-3.973869	2.676698
-1374.095048	0.429433	2.686694
-1372.477450	1.380076	2.696691
-1370.585216	0.900500	2.706688
-1368.420051	11.320441	2.716685
-1366.360973	2.562939	2.726682
-1364.763690	6.478816	2.736678
-1363.111405	4.918233	2.746675
-1361.284106	2.107583	2.756672
-1359.211376	0.815998	2.766669
-1357.219418	2.780362	2.776666
-1355.288419	-5.002982	2.786662
-1353.449462	3.887154	2.796659
-1351.678155	-7.516253	2.806656
-1349.779650	1.228568	2.816653
-1347.925488	-1.850044	2.826650
-1345.979483	9.203397	2.836646
-1344.105533	10.285123	2.846643
-1342.224572	11.733608	2.856640
-1340.511185	8.057034	2.866637
-1338.479410	-3.632788	2.876634
-1336.502608	3.556950	2.886630
-1334.929638	4.757911	2.896627
-1333.123569	5.553683	2.906624
-1331.046327	5.439245	2.916621
-1328.836571	2.873702	2.926618
-1327.377473	-0.841101	2.936614
-1325.281560	4.963853	2.946611
-1323.655365	7.239413	2.956608
-1321.621353	7.177691	2.966605
-1319.866922	6.218130	2.976602
-1317.803942	4.937616	2.986598
-1316.119128	12.219901	2.996595
-1314.008253	4.159908	3.006592
-1312.304323	4.454172	3.016589
-1310.241156	-0.568309	3.026586
-1308.540990	-0.575006	3.036582
-1306.836701	6.588909	3.046579
-1304.890057	5.492809	3.056576
-1302.558215	1.155194	3.066573
-1301.184760	12.087171	3.076570
-1298.884938	6.486842	3.086566
-1297.181687	6.909115	3.096563
-1295.402387	12.597415	3.106560
-1293.378949	11.009053	3.116557
-1291.491183	9.401357	3.126554
-1289.775251	7.799061	3.136550
-1287.911616	6.332592	3.146547
-1286.254009	10.433076	3.156544
-1284.113864	12.335895	3.166541
-1282.139076	9.294865	3.176538
-1280.385686	8.327605	3.186534
-1278.212035	4.643725	3.196531
-1276.410262	7.118579	3.206528
-1274.801190	14.408284	3.216525
-1272.926437	8.607599	3.226522
-1271.092075	8.066316	3.236518
-1268.948361	4.960369	3.246515
-1267.228030	6.901971	3.256512
-1265.234703	5.387924	3.266509
-1263.424878	4.468485	3.276506
-1261.775214	8.930243	3.286502
-1259.814772	9.908200	3.296499
-1257.436910	6.504275	3.306496
-1255.688603	8.899285	3.316493
-1254.174240	5.519875	3.326490
-1252.058846	8.032975	3.336486
-1250.349418	14.678245	3.346483
-1248.684232	9.275837	3.356480
-1246.555467	9.930039	3.366477
-1244.575299	3.296225	3.376474
-1242.885874	2.670795	3.386470
-1240.696279	9.908674	3.396467
-1238.838322	9.641524	3.406464
-1237.556735	0.160687	3.416461
-1235.616065	3.679089	3.426458
-1233.251915	12.014786	3.436454
-1231.406509	15.107932	3.446451
-1229.376874	15.452764	3.456448
-1228.048743	4.990309	3.466445
-1225.854279	8.900722	3.476442
-1224.129006	18.870183	3.486438
-1222.458762	8.771387	3.496435
-1219.983603	20.954442	3.506432
-1218.114104	13.411550	3.516429
-1216.660697	12.988110	3.526426
-1214.456449	13.336591	3.536422
-1212.915101	10.012885	3.546419
-1211.012103	9.097523	3.556416
-1209.096412	14.565132	3.566413
-1206.991442	6.034084	3.576410
-1205.096854	13.128163	3.586406
-1203.406142	10.150021	3.596403
-1201.412755	11.316959	3.606400
-1199.732410	9.508851	3.616397
-1197.675728	9.843067	3.626394
-1195.869721	13.766723	3.636390
-1194.163869	8.739934	3.646387
-1192.122879	7.417260	3.656384
-1190.128200	10.552868	3.666381
-1188.535347	6.366761	3.676378
-1186.677466	7.399085	3.686374
-1184.380841	7.420194	3.696371
-1182.940692	15.505916	3.706368
-1180.826956	11.411725	3.716365
-1178.887856	13.781005	3.726362
-1176.945430	5.069157	3.736358
-1175.193373	16.899032	3.746355
-1173.535702	14.663535	3.756352
-1171.516427	15.089020	3.766349
-1169.388149	12.396139	3.776346
-1167.693608	9.223207	3.786342
-1165.734729	11.167771	3.796339
-1164.010642	10.806841	3.806336
-1162.300762	7.647247	3.816333
-1160.476089	3.556695	3.826330
-1158.322781	5.858562	3.836326
-1156.524293	8.643499	3.846323
-1154.541555	12.466284	3.856320
-1152.484048	11.464673	3.866317
-1150.765364	9.822564	3.876314
-1149.073824	16.453411	3.886310
-1147.282755	7.535282	3.896307
-1145.318021	13.279299	3.906304
-1142.902042	4.169621	3.916301
-1141.350525	9.926067	3.926298
-1139.647321	10.042161	3.936294
-1137.836352	4.071790	3.946291
-1136.234439	10.319105	3.956288
-1133.888407	8.772423	3.966285
-1131.958052	9.663728	3.976282
-1130.272397	13.415647	3.986278
-1128.375081	9.624536	3.996275
-1126.348424	13.375586	4.006272
-1124.420135	4.171848	4.016269
-1122.678411	13.289321	4.026266
-1120.858180	9.497916	4.036262
-1119.019818	13.610662	4.046259
-1116.805523	5.014832	4.056256
-1115.242681	16.038223	4.066253
-1113.507065	6.579536	4.076250
-1111.510348	2.445709	4.086246
-1109.601469	19.342455	4.096243
-1107.588027	11.896611	4.106240
-1105.772863	8.803895	4.116237
-1103.934274	17.785896	4.126234
-1102.164436	6.674966	4.136230
-1100.111767	17.970524	4.146227
-1098.390310	8.345170	4.156224
-1096.158227	11.131844	4.166221
-1094.488032	3.699872	4.176218
-1092.299217	17.305669	4.186214
-1090.902004	15.283992	4.196211
-1089.143065	14.873333	4.206208
-1087.296146	16.480626	4.216205
-1085.386149	12.745937	4.226202
-1083.073372	17.940148	4.236198
-1081.410376	10.711429	4.246195
-1079.597638	6.995462	4.256192
-1077.560180	5.335571	4.266189
-1075.499558	10.071194	4.276186
-1073.719226	6.829343	4.286182
-1071.851098	11.995219	4.296179
-1070.250271	18.736952	4.306176
-1068.402783	-0.816039	4.316173
-1066.615826	9.216312	4.326170
-1064.465653	8.975187	4.336166
-1062.502345	5.451456	4.346163
-1060.638698	5.470894	4.356160
-1059.072659	4.187991	4.366157
-1056.890946	16.089767	4.376154
-1055.015177	14.937317	4.386150
-1053.451514	10.047045	4.396147
-1051.420675	6.870928	4.406144
-1049.185922	5.664222	4.416141
-1047.763110	9.475612	4.426138
-1045.829411	13.415281	4.436134
-1043.650275	11.285934	4.446131
-1042.310617	11.946543	4.456128
-1040.134238	9.209769	4.466125
-1038.267386	7.318262	4.476122
-1036.606206	6.179624	4.486118
-1034.591602	13.384127	4.496115
-1032.513162	10.487768	4.506112
-1030.794130	14.477574	4.516109
-1028.796523	9.778428	4.526106
-1027.151637	7.911379	4.536102
-1025.032498	8.164709	4.546099
-1023.210650	7.734564	4.556096
-1021.321653	-0.501271	4.566093
-1019.595089	3.285238	4.576090
-1017.191966	1.481657	4.586086
-1015.939001	5.880735	4.596083
-1013.885628	12.164883	4.606080
-1011.811972	10.939767	4.616077
-1010.126981	3.524429	4.626074
-1008.252287	7.501986	4.636070
-1006.430908	8.153466	4.646067
-1004.515548	10.359330	4.656064
-1002.700759	8.880371	4.666061
-1000.909965	7.209470	4.676058
-998.752284	9.501316	4.686054
-996.700981	8.372944	4.696051
-995.033394	10.558443	4.706048
-993.516768	9.766624	4.716045
-991.355559	-0.413702	4.726042
-989.274932	7.879187	4.736038
-987.419534	7.413706	4.746035
-985.713990	2.286060	4.756032
-984.184528	12.710177	4.766029
-981.957915	11.018538	4.776026
-979.860302	13.329483	4.786022
-977.942174	3.416977	4.796019
-976.591828	12.126654	4.806016
-974.499630	10.579671	4.816013
-972.549371	3.344559	4.826010
-970.509038	-0.031948	4.836006
-968.692722	14.001429	4.846003
-966.957826	11.144274	4.856000
-965.220302	9.221402	4.865997
-963.324190	9.826230	4.875994
-961.040254	4.801890	4.885990
-959.519558	5.785688	4.895987
-957.726158	9.640504	4.905984
-955.784756	12.557480	4.915981
-953.883523	6.839636	4.925978
-951.774918	1.748609	4.935974
-950.002442	6.970933	4.945971
-948.068520	12.862155	4.955968
-946.383440	9.046703	4.965965
-944.482129	5.866124	4.975962
-942.487072	9.551344	4.985958
-940.449525	12.355068	4.995955
-938.948931	11.229544	5.005952
-937.362485	17.937363	5.015949
-935.158656	20.297680	5.025946
-932.978611	14.824202	5.035942
-931.376377	17.249138	5.045939
-929.563098	20.882915	5.055936
-927.440685	13.792403	5.065933
-925.612811	6.381111	5.075930
-923.579609	13.742214	5.085926
-921.901791	16.545056	5.095923
-920.205078	20.042747	5.105920
-918.334099	19.483254	5.115917
-916.112832	11.794337	5.125914
-914.178947	8.771198	5.135910
-912.591137	13.887297	5.145907
-910.856565	17.574724	5.155904
-908.838244	18.554779	5.165901
-906.976333	17.344663	5.175898
-905.042000	21.178571	5.185894
-903.085034	15.175545	5.195891
-901.487038	12.394006	5.205888
-899.418169	12.691802	5.215885
-897.364581	19.103919	5.225882
-895.517174	12.052667	5.235878
-893.796993	15.930295	5.245875
-892.019040	20.199726	5.255872
-889.880625	17.898613	5.265869
-888.122103	13.850413	5.275866
-886.058103	10.871227	5.285862
-884.323616	11.580904	5.295859
-882.794813	9.012539	5.305856
-881.002231	14.545907	5.315853
-878.702652	17.383582	5.325850
-876.694229	8.505090	5.335846
-874.960120	12.424714	5.345843
-872.985775	17.422207	5.355840
-871.147159	9.579777	5.365837
-869.614795	10.403881	5.375834
-867.522669	5.558706	5.385830
-865.614964	18.912863	5.395827
-863.503158	7.546892	5.405824
-861.941198	13.729753	5.415821
-859.899831	13.946721	5.425818
-858.040569	10.520308	5.435814
-856.234762	8.761854	5.445811
-854.636786	10.573336	5.455808
-852.654933	10.784035	5.465805
-850.480133	5.650932	5.475802
-848.663900	9.017467	5.485798
-846.674757	16.641467	5.495795
-844.805623	14.427651	5.505792
-843.028494	18.551996	5.515789
-841.481579	12.500888	5.525786
-839.531055	20.194226	5.535782
-837.266261	18.264521	5.545779
-835.393180	13.945422	5.555776
-833.867706	12.433896	5.565773
-831.936961	9.973408	5.575770
-830.010910	11.004595	5.585766
-828.063267	7.455134	5.595763
-826.199410	18.539580	5.605760
-824.282881	12.146778	5.615757
-822.498935	11.266548	5.625754
-820.503956	10.674680	5.635750
-818.705676	17.468721	5.645747
-816.889408	12.926621	5.655744
-814.937445	6.802890	5.665741
-812.996376	11.123674	5.675738
-811.044684	17.714786	5.685734
-809.277553	9.615413	5.695731
-807.478088	18.521829	5.705728
-805.763120	15.020628	5.715725
-803.701989	13.541915	5.725722
-801.750429	12.001775	5.735718
-799.692944	19.812257	5.745715
-798.289048	16.259734	5.755712
-796.311315	11.838677	5.765709
-794.327636	8.226642	5.775706
-792.599239	7.858980	5.785702
-790.435422	7.492772	5.795699
-788.734558	12.271956	5.805696
-786.576731	18.639096	5.815693
-784.910712	13.985249	5.825690
-782.970344	12.737428	5.835686
-781.057515	14.163912	5.845683
-779.282560	11.947832	5.855680
-777.658733	12.721064	5.865677
-775.760869	6.399175	5.875674
-773.758050	10.929590	5.885670
-771.675871	8.896508	5.895667
-769.899685	14.787838	5.905664
-768.182854	17.788236	5.915661
-766.102829	11.827224	5.925658
-764.386308	10.487305	5.935654
-762.500255	7.697712	5.945651
-760.541684	7.493804	5.955648
-758.741417	7.686237	5.965645
-756.582688	12.240695	5.975642
-754.741813	10.869855	5.985638
-753.096273	3.661503	5.995635
-750.960485	7.682809	6.005632
-749.598404	9.645745	6.015629
-747.591855	14.041382	6.025626
-745.373370	4.115772	6.035622
-743.454400	6.875467	6.045619
-741.941283	4.990198	6.055616
-739.795092	9.421942	6.065613
-737.925788	11.786964	6.075610
-736.143505	15.271118	6.085606
-734.346192	11.909960	6.095603
-732.418645	1.928230	6.105600
-730.476728	19.107435	6.115597
-728.792624	11.390844	6.125594
-726.394704	8.768941	6.135590
-724.990374	9.455712	6.145587
-723.463412	12.595429	6.155584
-721.168959	9.214831	6.165581
-719.092539	12.326741	6.175578
-717.519083	11.136029	6.185574
-715.485304	3.159893	6.195571
-713.670811	9.659333	6.205568
-711.682911	7.723472	6.215565
-709.727683	11.330004	6.225562
-708.032595	3.280107	6.235558
-706.121687	4.443286	6.245555
-704.299946	11.167358	6.255552
-702.567498	5.301415	6.265549
-700.310835	5.957784	6.275546
-698.473789	7.956952	6.285542
-697.162950	6.505073	6.295539
-694.993686	11.359474	6.305536
-692.786976	2.324706	6.315533
-691.021705	4.426925	6.325530
-689.089038	4.797195	6.335526
-687.441939	3.850516	6.345523
-685.678777	4.371028	6.355520
-683.575554	4.433006	6.365517
-681.805858	8.583926	6.375514
-679.747941	2.803356	6.385510
-677.950287	2.579441	6.395507
-676.230983	17.171733	6.405504
-674.273002	11.321873	6.415501
-672.289803	6.437427	6.425498
-670.394441	12.404527	6.435494
-668.528653	14.310710	6.445491
-666.970390	7.741596	6.455488
-664.910964	3.705472	6.465485
-662.926883	2.597600	6.475482
-660.991592	5.755796	6.485478
-659.037375	3.517476	6.495475
-657.587355	10.706757	6.505472
-655.454162	10.091364	6.515469
-653.347238	4.081939	6.525466
-651.791583	9.081791	6.535462
-649.882733	7.307026	6.545459
-647.771943	9.033558	6.555456
-646.055814	7.043282	6.565453
-644.353053	5.773540	6.575450
-642.296995	8.618782	6.585446
-640.575100	9.011716	6.595443
-638.550811	7.490086	6.605440
-636.835522	8.184067	6.615437
-635.062967	8.988896	6.625434
-632.677111	8.977342	6.635430
-631.225080	11.129655	6.645427
-629.308624	11.753608	6.655424
-627.299679	3.170476	6.665421
-625.359746	5.009585	6.675418
-623.333644	7.224915	6.685414
-621.671798	8.465848	6.695411
-619.754190	7.562836	6.705408
-618.129961	5.928303	6.715405
-616.244292	9.457611	6.725402
-614.225153	6.537925	6.735398
-612.193544	8.016622	6.745395
-610.590879	6.169231	6.755392
-608.593345	5.536080	6.765389
-606.697578	12.330511	6.775386
-604.670215	8.190614	6.785382
-602.893582	3.495534	6.795379
-601.168101	9.050901	6.805376
-599.416812	11.019641	6.815373
-597.160488	11.292491	6.825370
-595.055894	5.378220	6.835366
-593.547567	7.308412	6.845363
-592.150586	11.566314	6.855360
-589.900187	14.895277	6.865357
-587.873144	6.749793	6.875354
-585.818006	5.030654	6.885350
-584.099212	13.725944	6.895347
-582.303811	9.173136	6.905344
-580.405659	6.828576	6.915341
-578.854651	3.090050	6.925338
-576.465518	5.826881	6.935334
-574.487775	2.948578	6.945331
-572.947778	9.883551	6.955328
-571.142302	9.882671	6.965325
-569.219352	14.274454	6.975322
-567.383233	8.309937	6.985318
-565.648430	6.588304	6.995315
-563.470110	8.466751	7.005312
-561.731946	7.852967	7.015309
-559.560186	8.756709	7.025306
-557.948728	11.721994	7.035302
-555.828014	4.392070	7.045299
-554.162598	7.678727	7.055296
-552.350539	11.568781	7.065293
-550.302656	13.139667	7.075290
-548.751045	11.489938	7.085286
-546.588529	9.598948	7.095283
-544.485280	10.655749	7.105280
-542.973558	8.347681	7.115277
-541.119246	10.885778	7.125274
-539.274652	7.381424	7.135270
-537.361313	13.596813	7.145267
-535.282504	12.742327	7.155264
-533.155474	11.101745	7.165261
-531.844803	12.479359	7.175258
-529.906725	11.985240	7.185254
-527.839767	10.908451	7.195251
-525.985316	9.895605	7.205248
-524.076561	16.013847	7.215245
-522.327380	10.538495	7.225242
-520.277038	14.010003	7.235238
-518.417114	6.096521	7.245235
-516.641314	9.376626	7.255232
-514.747397	11.253178	7.265229
-512.806946	8.780339	7.275226
-511.135133	3.224199	7.285222
-509.278709	14.281697	7.295219
-507.261211	15.186444	7.305216
-505.389666	9.541564	7.315213
-503.479331	11.282875	7.325210
-501.483584	13.446322	7.335206
-499.900902	9.694889	7.345203
-497.756457	19.293290	7.355200
-495.862505	12.969070	7.365197
-494.363013	16.591736	7.375194
-492.166833	9.169285	7.385190
-490.274025	14.500656	7.395187
-488.434663	16.357523	7.405184
-486.749846	9.948294	7.415181
-484.939029	13.495982	7.425178
-483.085814	5.503073	7.435174
-480.633696	0.021272	7.445171
-478.924787	1.351103	7.455168
-477.163382	13.800601	7.465165
-475.359957	14.059059	7.475162
-473.374448	5.454521	7.485158
-471.874824	16.624299	7.495155
-469.537110	7.219855	7.505152
-467.740602	13.221866	7.515149
-466.014052	17.477741	7.525146
-464.027219	5.862044	7.535142
-462.412022	7.437371	7.545139
-460.507538	7.992323	7.555136
-458.512097	10.408478	7.565133
-456.543978	11.400098	7.575130
-454.367512	0.530944	7.585126
-452.846465	7.753231	7.595123
-451.027050	17.373585	7.605120
-448.942139	19.197586	7.615117
-447.285451	8.417753	7.625114
-445.248520	14.431913	7.635110
-443.343334	9.410107	7.645107
-441.518715	10.126244	7.655104
-440.005274	11.953092	7.665101
-437.626563	5.011523	7.675098
-435.798927	14.755308	7.685094
-433.953865	4.261185	7.695091
-432.281694	14.418207	7.705088
-430.414026	4.051524	7.715085
-428.461519	13.423281	7.725082
-426.699133	2.163970	7.735078
-424.632238	11.054846	7.745075
-422.680014	12.413758	7.755072
-420.915862	14.525837	7.765069
-419.028211	14.564054	7.775066
-417.235882	3.465750	7.785062
-415.245261	0.727618	7.795059
-413.259019	3.445269	7.805056
-411.602169	9.044902	7.815053
-409.557825	10.812258	7.825050
-407.792963	8.446484	7.835046
-406.022123	3.185641	7.845043
-404.141224	10.108933	7.855040
-402.209027	4.296556	7.865037
-400.275774	4.278559	7.875034
-398.331756	8.826591	7.885030
-396.706793	5.436355	7.895027
-394.766782	2.657374	7.905024
-392.687674	9.755863	7.915021
-390.895797	4.797977	7.925018
-389.071178	2.967395	7.935014
-387.011895	4.702386	7.945011
-385.296000	2.238661	7.955008
-383.497139	7.689328	7.965005
-381.290208	-0.898389	7.975002
-379.618742	0.339600	7.984998
-378.079298	-0.583364	7.994995
-375.915559	0.032889	8.004992
-374.026500	5.066543	8.014989
-371.993232	2.458999	8.024986
-370.239059	7.263149	8.034982
-368.420083	-3.960948	8.044979
-366.501848	2.384851	8.054976
-364.681330	-2.516011	8.064973
-362.967472	4.686607	8.074970
-360.826674	2.447156	8.084966
-358.874753	2.055172	8.094963
-357.079069	10.428905	8.104960
-355.126508	0.571336	8.114957
-353.407931	4.493841	8.124954
-351.543264	6.533084	8.134950
-349.994511	11.627407	8.144947
-347.668202	5.692150	8.154944
-346.072237	5.524368	8.164941
-343.968855	8.911778	8.174938
-342.164536	8.196014	8.184934
-340.151041	6.886349	8.194931
-338.470425	6.101919	8.204928
-336.350037	2.302639	8.214925
-334.574808	12.719594	8.224922
-332.757733	8.814006	8.234918
-330.769471	3.046414	8.244915
-329.041806	1.048202	8.254912
-326.858135	10.722610	8.264909
-325.419738	2.008163	8.274906
-323.360713	4.450597	8.284902
-321.513133	-0.067726	8.294899
-319.686516	0.239251	8.304896
-317.786859	0.275630	8.314893
-315.695363	7.657993	8.324890
-313.915003	5.829795	8.334886
-312.263164	1.342727	8.344883
-310.098894	1.602124	8.354880
-308.257535	5.569798	8.364877
-306.475403	8.569591	8.374874
-304.613973	4.279588	8.384870
-302.612286	4.579156	8.394867
-300.671816	5.701631	8.404864
-299.264914	4.678299	8.414861
-297.321944	5.768800	8.424858
-295.233324	5.748191	8.434854
-293.231341	-0.312079	8.444851
-291.244976	-2.285247	8.454848
-289.451137	1.729500	8.464845
-287.680140	-2.535002	8.474842
-285.800450	-2.195420	8.484838
-284.047743	4.156349	8.494835
-282.129381	7.309673	8.504832
-280.275395	6.243407	8.514829
-278.252865	4.971823	8.524826
-276.343047	5.254499	8.534822
-274.668071	2.009512	8.544819
-272.779701	4.204503	8.554816
-270.650311	1.891163	8.564813
-269.241548	3.449050	8.574810
-267.098794	6.735511	8.584807
-265.329282	1.503396	8.594803
-263.319419	1.376969	8.604800
-261.306822	-1.617172	8.614797
-259.477243	2.852932	8.624794
-257.710116	5.072024	8.634791
-255.925084	-0.172035	8.644787
-253.595140	8.124404	8.654784
-252.040250	-6.562621	8.664781
-250.481393	5.890978	8.674778
-248.128353	2.653040	8.684775
-246.107544	-0.157668	8.694771
-245.105064	3.945529	8.704768
-242.825930	1.185168	8.714765
-240.902808	5.416154	8.724762
-238.686078	4.072555	8.734759
-237.058636	1.195169	8.744755
-235.169177	0.118538	8.754752
-233.585782	8.832564	8.764749
-231.447937	8.182067	8.774746
-229.230738	2.692214	8.784743
-227.747700	8.963916	8.794739
-225.649656	2.501535	8.804736
-224.143012	9.882596	8.814733
-222.015048	10.940475	8.824730
-219.954847	6.737226	8.834727
-217.973637	2.006603	8.844723
-216.148857	-1.274884	8.854720
-214.541657	3.630208	8.864717
-212.794406	4.987270	8.874714
-210.900319	6.025644	8.884711
-208.914040	-0.039950	8.894707
-206.993148	-1.484722	8.904704
-205.128343	-3.814197	8.914701
-203.355033	-0.020311	8.924698
-201.463074	3.224132	8.934695
-199.209228	1.895172	8.944691
-197.685051	1.587371	8.954688
-195.911429	2.607088	8.964685
-193.807468	2.688326	8.974682
-191.940935	10.300915	8.984679
-190.411596	5.983467	8.994675
-188.339333	5.130324	9.004672
-186.508863	-0.005679	9.014669
-184.571408	-6.404503	9.024666
-182.463445	1.392185	9.034663
-180.721269	-2.406605	9.044659
-179.139782	0.388470	9.054656
-177.104998	1.355472	9.064653
-175.144356	7.910982	9.074650
-173.157690	6.997303	9.084647
-171.319601	7.826757	9.094643
-169.364163	3.986046	9.104640
-167.782770	8.361624	9.114637
-165.972440	7.171362	9.124634
-163.906597	1.904660	9.134631
-161.784423	3.411923	9.144627
-160.317443	4.494810	9.154624
-158.321779	2.567632	9.164621
-156.411415	3.475562	9.174618
-154.322145	5.913319	9.184615
-152.413568	-0.204569	9.194611
-150.695535	7.403330	9.204608
-149.173582	2.733413	9.214605
-146.882110	-1.434050	9.224602
-145.103054	2.227916	9.234599
-143.305313	4.628520	9.244595
-141.315451	-0.389205	9.254592
-139.418548	0.418257	9.264589
-137.749068	2.037250	9.274586
-135.775410	-2.859467	9.284583
-133.745605	-0.686933	9.294579
-132.006039	0.456684	9.304576
-130.156608	-1.508715	9.314573
-128.341597	-1.629202	9.324570
-126.345607	-4.533744	9.334567
-124.417489	-2.798121	9.344563
-122.755679	3.366180	9.354560
-120.684137	7.695161	9.364557
-118.701924	11.105268	9.374554
-116.735839	15.664234	9.384551
-115.149570	3.798492	9.394547
-113.250773	7.228228	9.404544
-111.329215	6.915496	9.414541
-109.397673	3.801781	9.424538
-107.813543	5.137579	9.434535
-105.907960	2.130638	9.444531
-103.736059	3.421605	9.454528
-101.897075	4.383597	9.464525
-100.251864	4.200226	9.474522
-98.117521	4.811947	9.484519
-96.239799	9.841329	9.494515
-94.424843	14.206537	9.504512
-92.773732	16.281639	9.514509
-90.653894	16.946207	9.524506
-88.596382	13.826618	9.534503
-86.917311	17.872470	9.544499
-85.297679	16.194812	9.554496
-83.273106	17.660879	9.564493
-81.318515	9.735748	9.574490
-79.548323	14.674936	9.584487
-77.551689	13.155024	9.594483
-75.753446	14.980881	9.604480
-74.041197	14.461578	9.614477
-71.863277	11.123852	9.624474
-70.097426	10.550212	9.634471
-67.993011	14.256648	9.644467
-66.264987	17.017373	9.654464
-64.559001	15.119115	9.664461
-62.703131	17.134731	9.674458
-60.629869	12.935840	9.684455
-58.758191	15.656285	9.694451
-56.909072	14.510439	9.704448
-54.799926	15.056748	9.714445
-53.389876	18.215568	9.724442
-51.280973	16.759869	9.734439
-49.759063	15.140454	9.744435
-47.704282	13.450241	9.754432
-45.391193	14.865577	9.764429
-43.895257	10.926164	9.774426
-42.160870	14.361662	9.784423
-39.730758	18.025640	9.794419
-38.114880	21.694779	9.804416
-36.365789	17.713405	9.814413
-34.222611	15.124916	9.824410
-32.567935	16.642139	9.834407
-30.837549	16.535224	9.844403
-28.693222	9.885618	9.854400
-27.207311	14.052324	9.864397
-25.103387	13.405840	9.874394
-23.094620	13.197684	9.884391
-21.326575	13.986323	9.894387
-19.646056	12.234260	9.904384
-17.612292	16.067272	9.914381
-15.623820	13.599790	9.924378
-13.707315	20.664580	9.934375
-11.632956	14.750864	9.944371
-9.800291	11.277216	9.954368
-8.152322	14.819680	9.964365
-6.421809	6.407731	9.974362
-4.474267	10.900278	9.984359
-3.408608	33.960897	9.994355
-2.235496	82.290658	10.004352
-1.151626	139.246229	10.014349
0.000000	211.219283	10.019354
0.738128	250.112771	10.024359
1.016171	278.993808	10.029363
1.465593	324.428855	10.034368
2.198160	355.801616	10.039373
2.547698	389.306043	10.044378
3.060550	407.392100	10.049383
3.419101	414.968906	10.054387
3.434192	429.778685	10.059392
3.765776	432.793013	10.064397
3.532166	442.621529	10.069402
3.560823	465.113568	10.074407
3.880958	469.515856	10.079411
3.814822	478.492945	10.084416
3.998831	470.623163	10.089421
3.934127	486.024462	10.094426
3.946449	485.388657	10.099431
3.984648	482.375437	10.104435
4.214497	508.173825	10.109440
4.749840	506.926319	10.114445
4.329631	523.254833	10.119450
4.635623	522.078602	10.124455
5.006262	519.939588	10.129459
4.504102	508.203769	10.134464
4.522593	517.862815	10.139469
4.490388	517.171033	10.144474
4.393381	527.499784	10.149479
4.662674	535.276970	10.154483
4.725829	531.280478	10.159488
4.851989	525.126144	10.164493
4.852389	546.236686	10.169498
4.562589	546.669351	10.174503
5.122909	543.181754	10.179507
5.120780	539.887951	10.184512
5.007873	546.070317	10.189517
4.631871	544.523476	10.194522
4.888227	544.894257	10.199527
5.091113	551.393682	10.204531
5.033817	554.342332	10.209536
5.471921	566.615284	10.214541
5.417622	569.934042	10.219546
5.325526	569.136694	10.224551
5.713926	556.050846	10.229555
5.060918	571.530304	10.234560
5.448810	582.537106	10.239565
5.412531	599.066239	10.244570
5.359806	597.545098	10.249575
5.808940	584.514192	10.254579
5.506973	602.150146	10.259584
5.690353	606.285707	10.264589
5.914649	595.078915	10.269594
5.760347	603.824142	10.274599
5.647003	600.846107	10.279603
5.840379	602.113180	10.284608
5.917075	599.699343	10.289613
6.250549	614.590990	10.294618
6.032785	607.770813	10.299623
5.959571	607.828312	10.304627
5.750212	617.738232	10.309632
6.021582	601.502918	10.314637
5.809533	617.943414	10.319642
5.969584	621.824081	10.324647
6.030927	630.396155	10.329651
6.097000	641.623068	10.334656
6.374919	638.792351	10.339661
6.550124	647.950247	10.344666
6.590633	647.576444	10.349671
6.669497	659.066259	10.354675
6.748486	654.406463	10.359680
6.802671	654.181867	10.364685
6.829721	652.102370	10.369690
6.965593	658.243525	10.374695
6.860176	635.888187	10.379699
6.389469	644.007393	10.384704
6.662703	651.959055	10.389709
6.601693	659.306446	10.394714
6.570580	664.324638	10.399719
6.828120	657.997905	10.404723
6.588822	670.298569	10.409728
6.730387	661.675361	10.414733
6.991038	653.089934	10.419738
6.605986	665.246686	10.424743
7.179380	670.199997	10.429747
6.777154	680.140724	10.434752
7.185427	684.828641	10.439757
7.023412	697.891288	10.444762
7.557783	690.768175	10.449767
7.343473	690.988529	10.454771
7.282384	698.454223	10.459776
7.358191	691.251288	10.464781
7.469033	687.437959	10.469786
7.408347	693.066430	10.474791
7.663453	685.519507	10.479795
7.379399	700.561781	10.484800
7.839409	694.388818	10.489805
7.709364	694.613078	10.494810
7.806172	702.242824	10.499815
7.641432	705.927737	10.504819
7.305897	703.212204	10.509824
7.951253	716.997647	10.514829
7.952158	722.611575	10.519834
7.646792	735.567810	10.524839
7.863256	735.006666	10.529843
7.845206	737.419234	10.534848
8.077132	730.618735	10.539853
8.242699	733.511374	10.544858
8.089372	732.181308	10.549863
8.615773	724.862329	10.554867
8.349955	740.508867	10.559872
8.578203	733.144400	10.564877
8.804516	726.254911	10.569882
8.707803	733.677420	10.574887
8.921076	724.448222	10.579891
8.673125	741.260439	10.584896
9.199051	732.210027	10.589901
8.634975	716.044764	10.594906
8.824157	707.713556	10.599911
9.025564	701.730073	10.604915
8.516924	699.788054	10.609920
8.914081	705.368733	10.614925
8.957647	702.818237	10.619930
8.980989	702.674253	10.624935
8.967559	698.087532	10.629939
8.930663	709.411347	10.634944
8.801329	701.190873	10.639949
8.832901	706.992292	10.644954
8.912427	733.442690	10.649959
9.112162	723.854527	10.654963
9.003510	743.227592	10.659968
8.893025	740.824664	10.664973
9.222117	730.446305	10.669978
9.422702	735.531645	10.674983
9.543752	739.580992	10.679987
9.040172	741.019171	10.684992
9.407504	738.998925	10.689997
9.466285	746.544874	10.695002
9.197684	745.535971	10.700007
9.054868	740.553556	10.705011
9.039051	757.998975	10.710016
9.607301	760.942508	10.715021
9.919958	770.557955	10.720026
9.862192	781.582377	10.725031
9.937807	782.038765	10.730035
9.700556	785.090284	10.735040
9.714962	784.980841	10.740045
9.566374	785.061402	10.745050
9.664900	792.545840	10.750055
9.890925	787.323225	10.755059
9.959850	790.549838	10.760064
10.051228	781.854139	10.765069
10.003560	791.083945	10.770074
9.904224	791.429465	10.775079
10.247817	786.095057	10.780083
9.999088	799.171627	10.785088
10.287371	807.658721	10.790093
10.470839	811.672901	10.795098
10.508941	825.996860	10.800103
11.031026	814.182576	10.805107
10.563509	805.169151	10.810112
10.148288	800.405208	10.815117
10.614473	804.533565	10.820122
10.501386	819.575501	10.825127
10.907031	815.987932	10.830131
10.719490	833.342560	10.835136
11.178422	821.454763	10.840141
10.696064	826.332096	10.845146
10.679591	831.266009	10.850151
11.174097	825.634698	10.855155
11.010967	823.191268	10.860160
11.134622	818.385522	10.865165
11.058505	813.015546	10.870170
10.974397	812.387224	10.875175
11.219884	815.740223	10.880179
11.179999	830.365212	10.885184
10.976849	825.944331	10.890189
11.339136	825.437197	10.895194
11.296898	828.894441	10.900199
11.133763	825.230433	10.905203
11.017996	817.323123	10.910208
10.869554	831.911812	10.915213
11.366021	824.539210	10.920218
11.419783	831.097241	10.925223
11.719015	827.911424	10.930227
11.394120	829.929821	10.935232
11.489412	830.039292	10.940237
11.419415	820.306429	10.945242
11.359459	842.015240	10.950247
11.662861	854.611125	10.955251
11.515652	855.054170	10.960256
11.984281	860.398003	10.965261
11.737798	852.877381	10.970266
11.635927	858.290132	10.975271
12.246056	862.867063	10.980275
11.656262	859.865621	10.985280
11.597327	860.382897	10.990285
11.794130	867.520534	10.995290
11.995995	884.177588	11.000295
12.535281	879.460071	11.005299
12.022834	885.720503	11.010304
12.381985	889.970038	11.015309
13.022335	890.506666	11.020314
12.492264	873.130989	11.025319
12.464734	865.351507	11.030323
12.147301	858.517146	11.035328
12.400287	860.332984	11.040333
12.653135	878.320754	11.045338
12.326555	895.166191	11.050343
12.698201	882.940601	11.055347
12.616309	894.913568	11.060352
12.916311	886.883132	11.065357
12.996006	892.208587	11.070362
12.961432	891.419393	11.075367
13.401989	881.600323	11.080371
12.714142	870.004214	11.085376
13.250802	869.270566	11.090381
12.922960	870.836846	11.095386
12.996464	870.811018	11.100391
13.295236	872.010842	11.105395
12.875832	873.572802	11.110400
13.071795	870.936467	11.115405
13.284744	891.674559	11.120410
13.177300	904.302903	11.125415
13.336156	890.363951	11.130419
13.137058	896.985999	11.135424
13.183079	900.541148	11.140429
13.432110	907.124838	11.145434
13.357219	903.579202	11.150439
13.294609	899.840793	11.155443
13.275313	899.230514	11.160448
13.332346	888.556387	11.165453
13.193710	918.978063	11.170458
13.215952	908.222736	11.175463
13.644801	901.411249	11.180467
13.493859	941.885041	11.185472
13.824779	920.159849	11.190477
13.959234	934.599437	11.195482
14.107683	933.975017	11.200487
14.026399	924.153996	11.205491
14.243148	925.631841	11.210496
14.096376	926.634648	11.215501
14.226974	924.819298	11.220506
14.204014	930.987481	11.225511
14.190016	938.310167	11.230515
14.098314	939.362539	11.235520
14.116227	941.305771	11.240525
13.915516	925.815613	11.245530
13.907646	932.448176	11.250535
14.495179	925.849492	11.255539
14.491071	941.514426	11.260544
14.670917	926.469780	11.265549
14.547300	932.906336	11.270554
14.471834	943.735004	11.275559
14.575969	932.905095	11.280563
14.439944	939.723686	11.285568
14.529016	949.261372	11.290573
14.776329	959.680593	11.295578
14.977623	971.070701	11.300583
15.379369	959.906290	11.305587
14.642079	955.680955	11.310592
14.584080	943.728852	11.315597
15.122468	946.525798	11.320602
14.875250	964.665978	11.325607
15.150585	957.183499	11.330611
15.336061	970.441706	11.335616
15.327909	970.134006	11.340621
15.340602	961.570600	11.345626
15.065779	971.197883	11.350631
15.252265	966.963975	11.355635
15.232167	967.568103	11.360640
15.643131	957.170217	11.365645
15.600841	960.704773	11.370650
15.275716	961.829072	11.375655
15.531206	954.950592	11.380659
15.501945	960.842242	11.385664
15.520371	963.237991	11.390669
15.537387	960.401519	11.395674
15.466714	960.285144	11.400679
15.778414	952.956143	11.405683
15.302237	964.403841	11.410688
15.681941	954.714279	11.415693
15.788945	957.955357	11.420698
15.580914	954.779458	11.425703
15.776328	956.664418	11.430707
15.783798	964.609757	11.435712
15.670053	974.503092	11.440717
16.188098	973.753485	11.445722
16.179587	992.405995	11.450727
16.350914	1007.459532	11.455731
16.063460	989.565611	11.460736
16.338019	990.628955	11.465741
16.262093	983.737090	11.470746
16.235979	992.228708	11.475751
16.539453	993.683265	11.480755
16.462039	996.411281	11.485760
16.431755	990.347938	11.490765
16.487525	996.322237	11.495770
16.377490	996.910748	11.500775
16.652583	984.889712	11.505779
16.141599	1002.414406	11.510784
16.438204	1000.769692	11.515789
16.740453	997.942912	11.520794
16.407274	996.532696	11.525799
16.796755	994.135137	11.530803
16.614863	1004.146598	11.535808
16.971961	1009.069872	11.540813
17.053997	1014.536928	11.545818
16.941157	1012.008171	11.550823
17.374702	1003.011752	11.555827
16.701928	998.012850	11.560832
16.996082	1009.905431	11.565837
17.296869	1022.799932	11.570842
16.742119	1025.600936	11.575847
17.045751	1025.588866	11.580851
17.235976	1031.656854	11.585856
17.604972	1022.240200	11.590861
17.612787	1025.978096	11.595866
17.598863	1022.138847	11.600871
17.777762	1014.673298	11.605875
17.735106	1018.759874	11.610880
17.831702	1015.672571	11.615885
17.948545	1012.602541	11.620890
17.543635	1003.230488	11.625895
17.620508	1000.559507	11.630899
17.857958	1014.881820	11.635904
17.841847	1018.038467	11.640909
17.685770	1006.124033	11.645914
17.442612	1021.787759	11.650919
18.092533	1027.504872	11.655923
17.843404	1030.115200	11.660928
17.897298	1032.793893	11.665933
18.100870	1011.273386	11.670938
18.040733	1033.252177	11.675943
17.985322	1021.059894	11.680947
18.056313	1030.983728	11.685952
18.039230	1020.879581	11.690957
18.102854	1023.550413	11.695962
17.991790	1034.290207	11.700967
18.005165	1021.009864	11.705971
18.282942	1033.165281	11.710976
18.165354	1043.967626	11.715981
18.751504	1048.089537	11.720986
18.427871	1056.764270	11.725991
18.354186	1051.385933	11.730995
18.646368	1053.995083	11.736000
18.300051	1057.750047	11.741005
18.682601	1056.039579	11.746010
18.634990	1047.988804	11.751015
18.949179	1043.039050	11.756019
19.047657	1055.519559	11.761024
18.998774	1053.078367	11.766029
19.263043	1056.237611	11.771034
19.037000	1052.104172	11.776039
18.994882	1052.919978	11.781043
18.962785	1056.970187	11.786048
18.755197	1054.342991	11.791053
19.325427	1055.578383	11.796058
18.781117	1065.874780	11.801063
19.173319	1059.365541	11.806067
19.093277	1069.758205	11.811072
18.705311	1069.086870	11.816077
18.757976	1066.260461	11.821082
19.286025	1087.206415	11.826087
19.492371	1090.953665	11.831091
19.729260	1092.623863	11.836096
19.662506	1091.477080	11.841101
19.948168	1080.641762	11.846106
19.637949	1088.631532	11.851111
20.228628	1082.218363	11.856115
19.733925	1070.142627	11.861120
19.585247	1059.293022	11.866125
19.788237	1058.301919	11.871130
19.769575	1075.146549	11.876135
19.959695	1081.378583	11.881139
19.839829	1090.719447	11.886144
20.033249	1083.357205	11.891149
20.042106	1078.150201	11.896154
20.085240	1087.312095	11.901159
20.317303	1084.018662	11.906163
19.944561	1090.971278	11.911168
20.168767	1087.303771	11.916173
20.343577	1090.950391	11.921178
20.214079	1095.238503	11.926183
20.280014	1080.902593	11.931187
20.365816	1085.577421	11.936192
20.616719	1083.208260	11.941197
20.421679	1083.665248	11.946202
20.251159	1088.718439	11.951207
20.461552	1077.740583	11.956211
20.230412	1089.922025	11.961216
20.105011	1084.320105	11.966221
20.434321	1082.249107	11.971226
20.482762	1094.419077	11.976231
20.725540	1101.904323	11.981235
21.022203	1116.149481	11.986240
20.781842	1100.555069	11.991245
20.953742	1107.384550	11.996250
20.853871	1110.983522	12.001255
21.179610	1105.732274	12.006259
21.309884	1103.189956	12.011264
21.157442	1104.177908	12.016269
21.242088	1095.871038	12.021274
20.890126	1086.067848	12.026279
21.166912	1080.089535	12.031283
20.743822	1076.148372	12.036288
21.119649	1084.635861	12.041293
21.416474	1087.586486	12.046298
21.452906	1104.446806	12.051303
21.263431	1084.192135	12.056307
21.080734	1079.452514	12.061312
21.239012	1082.365310	12.066317
21.197681	1080.760297	12.071322
21.175498	1079.609559	12.076327
21.285718	1076.756621	12.081331
21.004453	1087.529910	12.086336
20.907087	1079.968038	12.091341
21.305499	1076.337405	12.096346
20.925134	1082.556350	12.101351
21.335484	1076.799593	12.106355
21.576507	1073.440076	12.111360
21.207458	1077.247558	12.116365
21.234603	1079.938412	12.121370
21.178520	1082.267215	12.126375
21.285596	1079.266539	12.131379
21.160043	1084.943357	12.136384
21.291417	1081.962461	12.141389
21.437645	1081.030874	12.146394
20.883680	1091.210553	12.151399
21.042634	1083.275049	12.156403
21.069303	1083.004371	12.161408
21.069763	1088.064984	12.166413
21.351150	1092.306483	12.171418
21.428382	1080.499860	12.176423
21.233522	1073.316252	12.181427
20.899095	1070.095042	12.186432
21.150526	1062.015485	12.191437
21.458045	1064.724696	12.196442
20.938517	1062.017939	12.201447
20.956199	1064.312895	12.206451
20.927777	1066.476429	12.211456
20.965179	1068.361375	12.216461
21.082011	1080.046536	12.221466
20.927798	1095.995785	12.226471
21.593113	1084.554267	12.231475
21.039302	1078.538118	12.236480
21.142536	1070.307936	12.241485
21.116463	1061.545645	12.246490
20.778599	1061.077636	12.251495
21.114812	1059.600070	12.256499
21.015629	1084.258968	12.261504
20.917918	1085.813795	12.266509
21.121106	1094.349327	12.271514
21.189428	1088.675504	12.276519
21.316406	1082.531844	12.281523
21.247755	1086.714051	12.286528
21.008405	1092.915240	12.291533
21.305748	1084.030385	12.296538
21.121847	1077.431672	12.301543
21.103355	1064.551411	12.306547
21.099764	1063.471828	12.311552
21.077219	1057.959172	12.316557
21.218561	1063.202315	12.321562
21.091190	1063.039788	12.326567
20.951718	1054.199392	12.331571
21.147908	1075.794367	12.336576
21.185136	1086.537356	12.341581
21.190857	1066.436874	12.346586
20.961796	1061.960127	12.351591
21.332649	1063.250976	12.356595
20.896054	1069.947253	12.361600
21.111883	1069.152804	12.366605
21.099651	1063.975978	12.371610
20.585843	1077.160522	12.376615
21.351600	1085.426541	12.381619
21.406307	1102.837472	12.386624
21.221125	1089.584005	12.391629
21.485631	1071.518363	12.396634
21.457396	1075.853397	12.401639
21.061410	1072.590753	12.406643
21.243256	1069.260389	12.411648
21.330368	1071.951926	12.416653
21.460634	1073.106103	12.421658
20.964479	1065.679599	12.426663
21.235444	1066.065413	12.431667
21.395690	1074.591224	12.436672
21.311675	1081.177652	12.441677
20.966028	1060.579694	12.446682
21.078987	1074.448034	12.451687
20.875223	1068.477774	12.456691
20.948962	1079.152643	12.461696
21.171094	1072.492324	12.466701
21.370052	1070.248937	12.471706
21.150011	1081.573079	12.476711
21.057155	1069.631951	12.481715
21.186578	1069.606666	12.486720
20.933219	1074.934058	12.491725
21.384194	1067.787007	12.496730
21.393434	1073.050436	12.501735
21.204648	1071.397978	12.506739
21.305325	1080.547535	12.511744
21.174115	1062.872247	12.516749
21.274230	1040.951869	12.521754
21.083366	1051.042066	12.526759
21.121997	1047.380513	12.531763
20.925445	1037.850621	12.536768
20.875804	1045.152237	12.541773
21.110928	1064.235926	12.546778
21.306360	1072.245175	12.551783
20.972766	1065.306845	12.556787
21.057075	1064.878736	12.561792
21.129043	1065.958630	12.566797
21.504748	1066.037570	12.571802
20.874748	1055.132270	12.576807
21.133714	1043.003369	12.581811
21.134657	1046.103683	12.586816
20.818084	1044.072630	12.591821
21.181994	1052.199291	12.596826
21.290304	1059.606613	12.601831
21.321778	1048.371879	12.606835
21.091158	1046.257728	12.611840
21.186808	1043.378734	12.616845
21.144124	1037.684789	12.621850
21.110550	1055.021432	12.626855
21.066927	1050.750084	12.631859
21.348776	1038.328945	12.636864
21.180712	1051.936939	12.641869
21.300691	1052.714276	12.646874
21.047921	1048.553560	12.651879
21.238846	1038.835705	12.656883
21.087773	1035.294302	12.661888
21.054650	1049.492644	12.666893
21.159124	1036.927906	12.671898
21.012315	1050.253380	12.676903
21.413020	1043.149841	12.681907
21.375089	1043.758393	12.686912
21.179132	1049.288726	12.691917
21.378996	1039.531597	12.696922
21.256308	1045.778815	12.701927
21.522695	1039.595590	12.706931
21.443157	1046.766354	12.711936
21.058202	1035.385156	12.716941
21.245074	1009.705622	12.721946
21.019644	1015.690087	12.726951
20.747712	1014.779468	12.731955
21.165800	1030.448124	12.736960
21.491557	1032.536238	12.741965
21.021282	1016.593799	12.746970
20.564145	1016.354557	12.751975
20.971777	1033.130357	12.756979
21.119683	1040.707976	12.761984
20.787506	1036.534697	12.766989
21.471602	1042.065012	12.771994
20.838960	1051.126506	12.776999
21.186374	1041.271722	12.782003
21.519976	1048.663604	12.787008
21.135573	1061.000359	12.792013
21.094738	1040.226864	12.797018
20.991169	1054.340250	12.802023
21.519403	1049.233348	12.807027
21.238247	1041.424836	12.812032
20.850746	1030.217519	12.817037
21.219040	1020.649585	12.822042
21.110854	1029.480754	12.827047
21.036556	1022.574417	12.832051
20.917985	1026.267816	12.837056
21.114645	1038.554451	12.842061
21.525091	1036.336474	12.847066
21.080234	1042.045280	12.852071
20.839705	1031.615633	12.857075
21.226136	1026.491932	12.862080
20.785589	1029.355147	12.867085
20.937416	1039.586223	12.872090
20.700776	1066.239050	12.877095
20.830370	1053.675021	12.882099
21.139279	1062.871781	12.887104
21.053362	1063.746616	12.892109
20.873127	1047.910851	12.897114
20.966997	1072.285040	12.902119
21.272844	1062.794062	12.907123
21.525614	1058.825531	12.912128
21.026446	1063.330295	12.917133
21.302717	1053.221915	12.922138
21.591723	1068.020197	12.927143
21.617192	1056.060995	12.932147
21.386504	1020.897744	12.937152
21.108146	1028.494460	12.942157
21.373418	1026.455762	12.947162
21.091277	1026.278496	12.952167
20.806247	1005.924055	12.957171
21.102901	1023.865595	12.962176
20.808088	1033.067165	12.967181
21.086809	1015.560734	12.972186
20.947535	1022.383037	12.977191
20.793627	1034.187828	12.982195
21.073358	1042.163903	12.987200
20.856402	1051.271062	12.992205
20.925026	1053.734515	12.997210
21.081389	1055.863843	13.002215
21.117019	1066.572379	13.007219
21.187439	1063.858260	13.012224
21.083285	1075.174952	13.017229
21.507973	1055.061278	13.022234
21.352303	1059.713110	13.027239
21.162377	1056.103780	13.032243
21.103840	1044.960679	13.037248
20.930538	1051.772652	13.042253
21.363378	1047.545161	13.047258
21.093074	1055.217878	13.052263
21.062461	1028.778193	13.057267
20.805586	1029.610905	13.062272
21.121125	1047.178868	13.067277
21.592747	1050.495855	13.072282
21.090400	1047.538771	13.077287
20.995853	1046.755980	13.082291
21.268536	1027.348641	13.087296
20.948791	1036.262444	13.092301
20.985172	1033.555337	13.097306
21.022740	1040.098699	13.102311
21.189502	1030.156039	13.107315
21.022660	1029.635522	13.112320
20.987139	1038.871433	13.117325
21.317047	1055.542958	13.122330
21.085421	1043.902324	13.127335
20.915761	1034.144212	13.132339
20.950386	1054.969331	13.137344
21.471007	1058.942421	13.142349
21.413530	1044.965284	13.147354
21.170354	1048.369472	13.152359
21.266996	1031.708949	13.157363
21.402127	1030.402233	13.162368
21.424663	1056.039119	13.167373
21.533021	1048.639998	13.172378
21.352890	1033.873436	13.177383
21.463287	1039.347017	13.182387
21.585597	1029.226940	13.187392
20.937034	1019.436409	13.192397
20.894399	1021.034486	13.197402
20.860576	1037.521148	13.202407
20.928718	1041.941728	13.207411
21.016026	1035.741335	13.212416
21.170025	1035.314727	13.217421
21.254388	1034.803030	13.222426
21.015670	1042.503820	13.227431
20.994810	1046.716241	13.232435
21.250246	1044.846271	13.237440
21.030353	1044.895626	13.242445
21.521298	1027.530379	13.247450
20.869371	1033.887237	13.252455
20.804849	1050.230572	13.257459
21.254833	1047.039588	13.262464
20.809572	1045.994182	13.267469
20.804725	1040.678988	13.272474
20.882174	1042.049750	13.277479
21.077088	1043.475896	13.282483
21.022507	1044.757327	13.287488
21.078062	1040.009680	13.292493
21.015824	1033.246497	13.297498
20.923526	1045.017816	13.302503
20.803117	1045.357241	13.307507
21.215944	1037.073755	13.312512
21.011745	1050.179718	13.317517
21.148967	1040.792134	13.322522
21.046554	1027.370977	13.327527
21.251206	1044.738998	13.332531
21.367100	1044.338969	13.337536
21.200711	1050.498539	13.342541
21.400512	1043.293000	13.347546
21.124493	1047.345840	13.352551
20.858208	1050.157610	13.357555
21.349288	1047.319626	13.362560
21.161116	1052.102799	13.367565
21.546992	1041.682046	13.372570
21.069360	1052.849339	13.377575
21.449435	1047.534250	13.382579
21.191271	1050.317915	13.387584
21.079182	1047.872612	13.392589
21.328215	1045.882235	13.397594
20.935102	1049.316646	13.402599
21.389776	1050.070561	13.407603
21.703288	1043.700040	13.412608
21.021945	1034.463523	13.417613
21.097448	1025.275034	13.422618
20.896511	1027.300494	13.427623
20.879174	1028.631178	13.432627
20.757845	1024.225571	13.437632
20.776333	1057.222941	13.442637
21.311256	1048.118859	13.447642
21.063695	1054.482195	13.452647
20.953804	1051.164462	13.457651
20.837155	1055.628713	13.462656
20.759240	1068.935330	13.467661
21.178795	1057.824776	13.472666
21.072464	1060.161590	13.477671
21.235400	1053.561185	13.482675
20.902400	1059.230078	13.487680
20.663882	1067.856548	13.492685
21.126461	1051.719548	13.497690
21.306796	1054.363885	13.502695
21.221758	1055.134496	13.507699
21.311476	1060.015278	13.512704
21.316816	1060.137522	13.517709
21.053814	1059.203398	13.522714
21.180669	1061.840496	13.527719
21.078218	1066.893861	13.532723
20.910725	1063.675201	13.537728
21.327762	1057.608293	13.542733
21.317619	1060.316129	13.547738
21.169378	1056.167125	13.552743
20.876166	1053.119911	13.557747
21.115207	1055.218705	13.562752
21.057042	1057.017965	13.567757
21.405751	1051.342014	13.572762
21.318771	1061.193291	13.577767
21.125780	1056.089455	13.582771
21.179442	1052.983761	13.587776
21.029015	1061.969925	13.592781
21.422891	1046.793242	13.597786
21.482430	1053.199060	13.602791
20.962640	1047.205884	13.607795
20.865855	1032.624732	13.612800
21.060917	1039.966165	13.617805
21.077023	1053.243578	13.622810
21.244248	1059.788347	13.627815
21.118641	1050.814850	13.632819
21.080265	1033.680683	13.637824
20.704217	1044.412286	13.642829
21.310335	1046.534534	13.647834
21.404280	1058.517438	13.652839
21.318295	1050.900148	13.657843
21.139201	1025.968105	13.662848
21.108423	1035.386190	13.667853
21.240533	1031.288673	13.672858
21.072682	1035.980288	13.677863
21.284144	1033.207407	13.682867
21.325010	1022.475834	13.687872
20.833023	1043.115265	13.692877
21.164197	1030.855004	13.697882
21.319870	1035.258468	13.702887
21.086746	1024.660483	13.707891
21.101996	1029.412780	13.712896
21.088894	1039.059866	13.717901
21.111401	1013.171569	13.722906
20.688039	1052.616767	13.727911
20.715237	1031.900244	13.732915
21.271135	1029.077157	13.737920
21.032443	1044.104665	13.742925
21.157750	1045.404714	13.747930
21.166229	1033.404085	13.752935
21.345065	1033.407190	13.757939
21.556350	1023.536283	13.762944
21.063698	1040.271178	13.767949
21.283525	1035.874233	13.772954
20.914908	1048.850296	13.777959
21.126226	1045.068158	13.782963
21.264234	1038.173683	13.787968
21.139476	1042.647109	13.792973
21.262362	1029.197900	13.797978
21.066320	1036.082881	13.802983
21.008549	1034.830588	13.807987
21.231679	1037.707799	13.812992
20.818029	1029.286475	13.817997
21.518568	1032.002380	13.823002
21.302274	1037.649497	13.828007
21.221708	1039.010768	13.833011
21.478768	1027.314281	13.838016
21.240906	1032.488583	13.843021
21.216220	1042.498650	13.848026
21.064468	1052.264056	13.853031
21.326638	1040.191417	13.858035
21.308820	1034.884602	13.863040
21.269420	1022.986238	13.868045
21.303873	1018.287697	13.873050
21.105536	1007.778796	13.878055
20.964110	1004.354136	13.883059
20.863164	999.760778	13.888064
21.140811	1005.983550	13.893069
21.025098	1011.485300	13.898074
21.120885	1015.765842	13.903079
20.854876	1024.298897	13.908083
21.084235	1023.876039	13.913088
21.210694	1035.708655	13.918093
21.366158	1035.518364	13.923098
20.877842	1021.127408	13.928103
21.241705	1020.728830	13.933107
21.459938	1012.608863	13.938112
21.055845	1014.263015	13.943117
20.898803	1003.804302	13.948122
21.165160	1000.120632	13.953127
21.123608	995.166132	13.958131
21.113070	1000.928653	13.963136
20.925737	1000.759921	13.968141
21.253588	993.533982	13.973146
20.782494	1007.075147	13.978151
20.925933	1017.734911	13.983155
21.399002	1032.363445	13.988160
21.219120	1028.271537	13.993165
20.972701	1012.033194	13.998170
21.016003	1024.623406	14.003175
21.250075	1025.655363	14.008179
21.215273	1009.246072	14.013184
20.852041	1010.381183	14.018189
21.358446	1022.543803	14.023207
20.849165	1006.330719	14.028224
21.186439	1025.223447	14.033242
21.080335	1036.197786	14.038259
21.143073	1036.290112	14.043277
21.125198	1040.953773	14.048295
21.101099	1044.023432	14.053312
21.370149	1046.267712	14.058330
21.540482	1040.096597	14.063347
21.159179	1040.623105	14.068365
21.381556	1037.652556	14.073383
21.508522	1037.180951	14.078400
20.920788	1022.265482	14.083418
21.116656	1036.189741	14.088435
21.299676	1048.761731	14.093453
21.346932	1036.796536	14.098471
21.471864	1051.652314	14.103488
21.102505	1046.328597	14.108506
21.449666	1050.241929	14.113523
20.975504	1059.198665	14.118541
21.206219	1048.492465	14.123559
21.304861	1046.845647	14.128576
21.342078	1056.213157	14.133594
21.539578	1054.195077	14.138611
21.502563	1058.465406	14.143629
21.586439	1062.046367	14.148647
22.069470	1043.801552	14.153664
21.545466	1056.016000	14.158682
21.669677	1053.594345	14.163699
21.335826	1063.054077	14.168717
21.420796	1061.302475	14.173735
21.638251	1063.341063	14.178752
21.378056	1064.073190	14.183770
21.665103	1050.072058	14.188787
21.585465	1055.237915	14.193805
21.531832	1079.788138	14.198823
21.574647	1084.347754	14.203840
21.494887	1081.126522	14.208858
21.794453	1083.672671	14.213875
21.829550	1097.477918	14.218893
22.035421	1088.900748	14.223911
22.145073	1092.617599	14.228928
21.685708	1093.847097	14.233946
21.746035	1095.143137	14.238963
22.033955	1096.966003	14.243981
22.102479	1082.167588	14.248999
21.747881	1093.667656	14.254016
21.619826	1098.710694	14.259034
21.901086	1092.252885	14.264051
21.698001	1090.959345	14.269069
21.863694	1084.471210	14.274087
21.985534	1080.744356	14.279104
21.989046	1090.968246	14.284122
22.366908	1092.457451	14.289139
22.031957	1090.107452	14.294157
22.077815	1099.855846	14.299175
22.044807	1088.255758	14.304192
22.046700	1096.033928	14.309210
22.266150	1081.579518	14.314227
22.094790	1091.000767	14.319245
21.972400	1091.135205	14.324263
21.794729	1089.299653	14.329280
22.005290	1095.660318	14.334298
22.119882	1095.568200	14.339315
22.175069	1104.652098	14.344333
22.328736	1122.510904	14.349351
22.373641	1127.578273	14.354368
22.279549	1128.925687	14.359386
22.551585	1115.625291	14.364403
22.635925	1118.504641	14.369421
22.292496	1100.831225	14.374439
22.594988	1092.823789	14.379456
22.274147	1091.140057	14.384474
21.954420	1090.219042	14.389491
22.552441	1119.419722	14.394509
22.647025	1116.574931	14.399527
22.918092	1121.890935	14.404544
22.431994	1109.733905	14.409562
22.653424	1099.627669	14.414579
22.612946	1093.222749	14.419597
22.263321	1103.309496	14.424615
22.714294	1100.574600	14.429632
22.696006	1094.840949	14.434650
22.471317	1106.681305	14.439667
22.598224	1114.873688	14.444685
22.659210	1109.048738	14.449703
22.923469	1124.678296	14.454720
22.670335	1118.382787	14.459738
22.823464	1099.091795	14.464755
22.497607	1107.456273	14.469773
22.449501	1116.283742	14.474791
22.816034	1119.018985	14.479808
22.799508	1122.861360	14.484826
23.042447	1124.257261	14.489843
22.874801	1123.151542	14.494861
22.825840	1135.722858	14.499879
22.875685	1139.430385	14.504896
22.857739	1139.301206	14.509914
22.687642	1129.662441	14.514931
22.682021	1125.556368	14.519949
22.228541	1123.989739	14.524967
22.674543	1127.561720	14.529984
22.304632	1126.743085	14.535002
22.640446	1141.730482	14.540019
23.085525	1145.478789	14.545037
23.108819	1161.245918	14.550055
23.429623	1154.888737	14.555072
22.900119	1144.810224	14.560090
23.298435	1164.300570	14.565107
23.467949	1156.926201	14.570125
23.356783	1143.726225	14.575143
23.533813	1122.514708	14.580160
23.013434	1135.349971	14.585178
23.007364	1124.576094	14.590195
23.394835	1122.532424	14.595213
23.048790	1128.415608	14.600231
23.420266	1127.338727	14.605248
23.009986	1137.469778	14.610266
23.412393	1133.616365	14.615283
23.295095	1122.358448	14.620301
23.215871	1124.447510	14.625319
23.750297	1117.744822	14.630336
23.123955	1144.165544	14.635354
23.576748	1137.452273	14.640371
23.398771	1126.279534	14.645389
23.306100	1123.022600	14.650407
23.430105	1125.815404	14.655424
23.497991	1143.827914	14.660442
23.618773	1147.829288	14.665459
23.757027	1126.583052	14.670477
23.122681	1129.614787	14.675495
23.703302	1139.872500	14.680512
23.480738	1160.739135	14.685530
23.597201	1154.139274	14.690547
23.712111	1149.891277	14.695565
23.370810	1148.585171	14.700583
23.573516	1169.302193	14.705600
23.408586	1153.057614	14.710618
23.422063	1149.407801	14.715635
23.725049	1157.800206	14.720653
23.838748	1150.489798	14.725671
24.159779	1149.914879	14.730688
23.986184	1160.269309	14.735706
23.661647	1139.686739	14.740723
23.635948	1158.653266	14.745741
23.799544	1165.144146	14.750759
24.037111	1153.861063	14.755776
23.597481	1158.245974	14.760794
24.008764	1153.194098	14.765811
23.989849	1154.532669	14.770829
23.708541	1165.203151	14.775847
23.768794	1161.714183	14.780864
24.071313	1161.019523	14.785882
23.868046	1162.444127	14.790899
24.258933	1158.903996	14.795917
24.085571	1154.208059	14.800935
24.208129	1144.497438	14.805952
24.189318	1159.151316	14.810970
24.155312	1163.759388	14.815987
24.105249	1153.506872	14.821005
23.899881	1155.666395	14.826023
24.012243	1162.627903	14.831040
24.183075	1153.257206	14.836058
24.347306	1153.888609	14.841075
24.471711	1164.650105	14.846093
24.274379	1161.980850	14.851111
24.431844	1145.919233	14.856128
24.059350	1153.906581	14.861146
24.032376	1144.186778	14.866163
24.253645	1150.250038	14.871181
24.274184	1157.945044	14.876199
24.357076	1149.547898	14.881216
24.369409	1153.755330	14.886234
24.318728	1153.011615	14.891251
24.153892	1150.094940	14.896269
24.315836	1166.439268	14.901287
24.657019	1174.523577	14.906304
24.956877	1176.638698	14.911322
24.609908	1172.892216	14.916339
24.746170	1148.542761	14.921357
24.388734	1150.858668	14.926375
24.491424	1154.106324	14.931392
24.324928	1161.052536	14.936410
24.571867	1164.964582	14.941427
24.794369	1172.835017	14.946445
24.598158	1194.186696	14.951463
24.883170	1174.705472	14.956480
24.797020	1177.487761	14.961498
24.826157	1175.829993	14.966515
25.031693	1154.294566	14.971533
24.871838	1156.077177	14.976551
24.595286	1150.966702	14.981568
24.999712	1151.408787	14.986586
24.573859	1143.487608	14.991603
24.972187	1150.721242	14.996621
24.448900	1165.505925	15.001639
25.028754	1164.688382	15.006656
25.060584	1182.219064	15.011674
24.918134	1180.900115	15.016691
25.104391	1176.329278	15.021709
25.041412	1191.768863	15.026727
24.994415	1184.218234	15.031744
24.993883	1173.625903	15.036762
24.892655	1171.084459	15.041779
25.261976	1190.426886	15.046797
25.141575	1175.295149	15.051815
25.313286	1162.145989	15.056832
25.078308	1180.996491	15.061850
24.866304	1185.859471	15.066867
25.367888	1172.590049	15.071885
25.013419	1181.431816	15.076903
25.173185	1174.132924	15.081920
25.305224	1174.552390	15.086938
25.038948	1174.690902	15.091955
25.361169	1177.216153	15.096973
25.212618	1181.466556	15.101991
25.193977	1182.389817	15.107008
25.341633	1181.192906	15.112026
25.351495	1187.919097	15.117043
25.355607	1176.413689	15.122061
25.152247	1180.427448	15.127079
25.082338	1172.073536	15.132096
25.375642	1174.323406	15.137114
25.501258	1184.474405	15.142131
25.721273	1172.846476	15.147149
25.530708	1183.191046	15.152167
25.401394	1175.441197	15.157184
25.813204	1178.170803	15.162202
25.400325	1183.655693	15.167219
25.702933	1174.259245	15.172237
25.464891	1189.179350	15.177255
25.476147	1180.321715	15.182272
25.423032	1185.713044	15.187290
25.651459	1202.981166	15.192307
25.978879	1198.854985	15.197325
25.699663	1213.698313	15.202343
26.025470	1203.444012	15.207360
26.441148	1192.969322	15.212378
25.838615	1179.622747	15.217395
26.053310	1174.830303	15.222413
25.636108	1170.942444	15.227431
25.774336	1173.009414	15.232448
26.006510	1178.476358	15.237466
25.567866	1176.457482	15.242483
25.805349	1182.453677	15.247501
25.852450	1198.891863	15.252519
25.888595	1195.189659	15.257536
25.999925	1204.943411	15.262554
25.885278	1195.789676	15.267571
26.171882	1203.292836	15.272589
26.190879	1196.178404	15.277607
26.438341	1196.854734	15.282624
26.212135	1197.513807	15.287642
26.529068	1206.830508	15.292659
26.623217	1181.378756	15.297677
26.193922	1178.664700	15.302695
26.111913	1171.498751	15.307712
26.222026	1163.499940	15.312730
25.982108	1166.563150	15.317747
26.100253	1180.688704	15.322765
26.182073	1187.389260	15.327783
26.155758	1186.467056	15.332800
26.422823	1190.509603	15.337818
26.328647	1199.327167	15.342835
26.593173	1190.070488	15.347853
26.479095	1200.874768	15.352871
26.386842	1187.182534	15.357888
26.338073	1187.215570	15.362906
26.271521	1197.044878	15.367923
26.247633	1186.322559	15.372941
26.260524	1192.134362	15.377959
26.333019	1190.917978	15.382976
26.511392	1193.396963	15.387994
26.071452	1198.238102	15.393011
26.719370	1205.755992	15.398029
26.346270	1217.101808	15.403047
26.802558	1221.030814	15.408064
26.985760	1227.216581	15.413082
26.948454	1216.004033	15.418099
26.984722	1204.767174	15.423117
27.076989	1196.863998	15.428135
26.712813	1192.237807	15.433152
27.070616	1180.048360	15.438170
26.968791	1179.635265	15.443187
27.103012	1181.650967	15.448205
26.963196	1198.381654	15.453223
26.672206	1191.870359	15.458240
26.934148	1187.753052	15.463258
26.757921	1186.168935	15.468275
26.950138	1186.043987	15.473293
26.923254	1182.310942	15.478311
26.687250	1188.016154	15.483328
26.969939	1199.004108	15.488346
26.982916	1213.259723	15.493363
26.999292	1213.790445	15.498381
27.269588	1215.388054	15.503399
27.196652	1223.867197	15.508416
27.271769	1217.454797	15.513434
27.410394	1225.046063	15.518451
27.257510	1211.363477	15.523469
27.381218	1213.385579	15.528487
27.201642	1213.201956	15.533504
27.222399	1216.892121	15.538522
27.104840	1203.576708	15.543539
27.130884	1220.078050	15.548557
27.047536	1221.061970	15.553575
26.963546	1220.570525	15.558592
27.195007	1220.997730	15.563610
27.404100	1214.899009	15.568627
27.446030	1213.454695	15.573645
27.487120	1205.934048	15.578663
27.604122	1218.118750	15.583680
27.653640	1202.727079	15.588698
27.430560	1214.568053	15.593715
27.687723	1205.447815	15.598733
27.833521	1210.744508	15.603751
27.631981	1218.117899	15.608768
27.652505	1206.240196	15.613786
27.652161	1216.183224	15.618803
27.349709	1214.787546	15.623821
27.454665	1202.356844	15.628839
27.631348	1218.420461	15.633856
27.969197	1219.321471	15.638874
27.563887	1224.350573	15.643891
28.049652	1224.041954	15.648909
28.297426	1232.823874	15.653927
27.778299	1221.689744	15.658944
27.925699	1209.862587	15.663962
27.863368	1215.744598	15.668979
27.931243	1209.283020	15.673997
27.896931	1207.006171	15.679015
28.037224	1225.542051	15.684032
28.301721	1217.559484	15.689050
27.851373	1214.891250	15.694067
27.761884	1221.505890	15.699085
28.427278	1220.927953	15.704103
27.948909	1226.423303	15.709120
28.141497	1212.265625	15.714138
28.348154	1234.355333	15.719155
28.167466	1229.729751	15.724173
28.671730	1229.564470	15.729191
28.242069	1216.372755	15.734208
28.106416	1194.951460	15.739226
28.074762	1215.591100	15.744243
28.376729	1213.298366	15.749261
28.247145	1232.896600	15.754279
28.151992	1234.620138	15.759296
28.788161	1225.661230	15.764314
28.853363	1226.925045	15.769331
28.287863	1218.687903	15.774349
28.585921	1212.519938	15.779367
28.635284	1207.162409	15.784384
28.416266	1203.047879	15.789402
28.081438	1218.861181	15.794419
28.467852	1218.440996	15.799437
28.878128	1227.185983	15.804455
28.768895	1241.668753	15.809472
28.960009	1226.072006	15.814490
28.767402	1216.233856	15.819507
28.514725	1204.328946	15.824525
28.863901	1210.117006	15.829543
28.680414	1213.405601	15.834560
28.850968	1198.342262	15.839578
28.778297	1212.542325	15.844595
28.729445	1204.125262	15.849613
29.077810	1201.345367	15.854631
28.773160	1205.724492	15.859648
28.874761	1199.603598	15.864666
29.271216	1209.694113	15.869683
28.296347	1215.455836	15.874701
28.731891	1221.431469	15.879719
28.953740	1231.527827	15.884736
29.385262	1230.128337	15.889754
29.251976	1227.165715	15.894771
29.101550	1231.800242	15.899789
29.017766	1228.545013	15.904807
29.030240	1233.763881	15.909824
29.107281	1242.810561	15.914842
29.061497	1235.868460	15.919859
28.737190	1228.388778	15.924877
29.107223	1228.296816	15.929895
29.183629	1240.753847	15.934912
29.116080	1228.822535	15.939930
29.085575	1246.495369	15.944947
28.849894	1237.008562	15.949965
29.245697	1228.490676	15.954983
29.217277	1245.455330	15.960000
29.263891	1254.061712	15.965018
29.569339	1251.397190	15.970035
29.489611	1264.041163	15.975053
29.305900	1268.891792	15.980071
29.338775	1270.145037	15.985088
29.632236	1273.395325	15.990106
29.282573	1267.588619	15.995123
28.943831	1275.856936	16.000141
29.387350	1268.528469	16.005159
29.184845	1270.011162	16.010176
29.229715	1273.911424	16.015194
29.629005	1279.707249	16.020211
29.709258	1278.988262	16.025229
29.757434	1287.677784	16.030247
29.609036	1294.138261	16.035264
29.824172	1286.237461	16.040282
29.975312	1290.792448	16.045299
29.709786	1292.228567	16.050317
30.172581	1280.193748	16.055335
29.831238	1293.623502	16.060352
29.794902	1287.063682	16.065370
30.075384	1280.585465	16.070387
29.900721	1277.849653	16.075405
29.903078	1277.577237	16.080423
30.029260	1284.429637	16.085440
30.309568	1288.013929	16.090458
30.279156	1288.399535	16.095475
30.020741	1291.308421	16.100493
30.466068	1272.672939	16.105511
30.238154	1288.156236	16.110528
30.484226	1284.826361	16.115546
30.477839	1262.283249	16.120563
30.120677	1276.409203	16.125581
30.222788	1256.043129	16.130599
29.952787	1260.585055	16.135616
30.233139	1277.576002	16.140634
30.541779	1273.753239	16.145651
30.161554	1293.427709	16.150669
30.741332	1280.515374	16.155687
30.396526	1284.491947	16.160704
30.288509	1284.883639	16.165722
30.502194	1276.734541	16.170739
30.101048	1284.015533	16.175757
30.206984	1283.575589	16.180775
30.235345	1290.443594	16.185792
30.316436	1283.555165	16.190810
30.500680	1279.596515	16.195827
30.599156	1278.212388	16.200845
30.811458	1283.180754	16.205863
30.728549	1285.946818	16.210880
30.748308	1281.353742	16.215898
30.912459	1277.218975	16.220915
30.704968	1277.680014	16.225933
30.837258	1275.279056	16.230951
30.602457	1288.948211	16.235968
30.919181	1286.351097	16.240986
30.680222	1286.724348	16.246003
30.994380	1300.261913	16.251021
31.158474	1301.113565	16.256039
31.197607	1297.785233	16.261056
31.233875	1286.549885	16.266074
31.124640	1269.188900	16.271091
30.915900	1267.866358	16.276109
31.082844	1272.974087	16.281127
31.143744	1280.757102	16.286144
31.266389	1267.249164	16.291162
31.306635	1267.132724	16.296179
31.056721	1271.855490	16.301197
31.525588	1265.325212	16.306215
31.363430	1265.686213	16.311232
31.222842	1266.435451	16.316250
31.321986	1270.163463	16.321267
31.113556	1283.068649	16.326285
31.328397	1259.697464	16.331303
31.322504	1268.249309	16.336320
31.170121	1275.846119	16.341338
31.585540	1280.484792	16.346355
31.527324	1300.951041	16.351373
32.173319	1294.276097	16.356391
31.708014	1279.957447	16.361408
31.408682	1271.369513	16.366426
31.936163	1260.541895	16.371443
31.543638	1262.103657	16.376461
31.798329	1259.190830	16.381479
31.753715	1268.846805	16.386496
31.608130	1273.491584	16.391514
31.674581	1260.615522	16.396531
31.438707	1272.235218	16.401549
31.421124	1267.880906	16.406567
31.669248	1284.714983	16.411584
31.894101	1298.840936	16.416602
32.071379	1295.640006	16.421619
32.187446	1303.123228	16.426637
31.834345	1285.368544	16.431655
31.964390	1298.617727	16.436672
32.144113	1295.388093	16.441690
32.132543	1297.843910	16.446707
31.843248	1292.420815	16.451725
32.027312	1297.310322	16.456743
32.168663	1297.103825	16.461760
32.002999	1302.775841	16.466778
32.111652	1306.794924	16.471795
32.293292	1300.661221	16.476813
32.231168	1296.428834	16.481831
32.253060	1295.951958	16.486848
32.258946	1300.130574	16.491866
32.337233	1301.167369	16.496883
32.171758	1305.327700	16.501901
32.105110	1295.702211	16.506919
32.191670	1301.349727	16.511936
32.083788	1300.309965	16.516954
32.233543	1294.719317	16.521971
32.133353	1296.722087	16.526989
31.932936	1303.607711	16.532007
32.179341	1304.677466	16.537024
32.523139	1328.426984	16.542042
32.838421	1318.223044	16.547059
32.740540	1328.974500	16.552077
32.744914	1324.420043	16.557095
32.519219	1331.636896	16.562112
32.566027	1328.927097	16.567130
32.563856	1336.740650	16.572147
32.715056	1320.387261	16.577165
32.787516	1324.128981	16.582183
32.710291	1326.854820	16.587200
32.790321	1316.677392	16.592218
32.946839	1313.088092	16.597235
32.923845	1326.729793	16.602253
33.139356	1325.618001	16.607271
33.092016	1317.357931	16.612288
32.832290	1325.918836	16.617306
32.988025	1311.268297	16.622323
32.845830	1321.798730	16.627341
32.665184	1323.222886	16.632359
33.086164	1308.419934	16.637376
33.011039	1316.537691	16.642394
32.940205	1310.804470	16.647411
32.855646	1334.439850	16.652429
32.852223	1345.374451	16.657447
33.369977	1343.168402	16.662464
33.251751	1343.102405	16.667482
33.578965	1355.239537	16.672499
33.540819	1350.194784	16.677517
33.623619	1350.519864	16.682535
33.701535	1352.119858	16.687552
33.519745	1346.701618	16.692570
33.637043	1343.749342	16.697587
33.336620	1341.706822	16.702605
33.674133	1344.364942	16.707623
33.588598	1346.208081	16.712640
33.545300	1348.969411	16.717658
33.900039	1348.799665	16.722675
33.724732	1351.931258	16.727693
33.817469	1344.548592	16.732711
33.867032	1324.192377	16.737728
33.491271	1311.369498	16.742746
33.731753	1332.439374	16.747763
33.621706	1348.150898	16.752781
33.554595	1351.472871	16.757799
33.819541	1353.848415	16.762816
33.706731	1345.575176	16.767834
34.007194	1348.029997	16.772851
33.838382	1343.770568	16.777869
33.908600	1343.561259	16.782887
33.880511	1340.426108	16.787904
33.592483	1357.572296	16.792922
34.144290	1350.319325	16.797939
33.770894	1344.934792	16.802957
33.439850	1350.093662	16.807975
33.848967	1363.067161	16.812992
33.842033	1370.747787	16.818010
34.249241	1369.468565	16.823027
34.281299	1387.883492	16.828045
34.171376	1385.033514	16.833063
34.580458	1369.892627	16.838080
34.329691	1374.673764	16.843098
34.488380	1378.821739	16.848115
34.449915	1371.810766	16.853133
34.581576	1377.716957	16.858151
34.927460	1373.820589	16.863168
34.869598	1379.050727	16.868186
34.712619	1381.358292	16.873203
34.993763	1376.342828	16.878221
34.813079	1363.122278	16.883239
34.699151	1350.418050	16.888256
34.532352	1350.455754	16.893274
34.317805	1337.102204	16.898291
34.567465	1351.617504	16.903309
34.005475	1367.421580	16.908327
34.878242	1365.017334	16.913344
34.921341	1371.604604	16.918362
34.890621	1366.330574	16.923379
34.805591	1372.305930	16.928397
34.668359	1376.538855	16.933415
35.078626	1365.728281	16.938432
35.012355	1375.126660	16.943450
35.181915	1360.354318	16.948467
34.884619	1364.593893	16.953485
35.089778	1368.147720	16.958503
35.093187	1365.056303	16.963520
35.065171	1369.160123	16.968538
34.948090	1362.455846	16.973555
35.104101	1359.638962	16.978573
34.659536	1366.546253	16.983591
35.470550	1371.977578	16.988608
35.313853	1395.901413	16.993626
35.503294	1403.676576	16.998643
35.720177	1383.343928	17.003661
35.415128	1383.405255	17.008679
35.437733	1365.927173	17.013696
34.988225	1377.872032	17.018714
35.646527	1386.870139	17.023731
35.739715	1398.402845	17.028749
35.586567	1398.578370	17.033767
36.167145	1380.814649	17.038784
35.843295	1375.065129	17.043802
35.698551	1363.731177	17.048819
35.791760	1355.635856	17.053837
35.538365	1364.395546	17.058855
35.632289	1356.440109	17.063872
35.440364	1356.576201	17.068890
35.493933	1363.221571	17.073907
35.740176	1386.593492	17.078925
35.787127	1399.591755	17.083943
35.877080	1389.080788	17.088960
35.733827	1395.084316	17.093978
35.834685	1393.770584	17.098995
36.094294	1398.116399	17.104013
35.657910	1390.173166	17.109031
35.587193	1394.058862	17.114048
35.911572	1398.252775	17.119066
36.106039	1397.188378	17.124083
36.014362	1397.310054	17.129101
35.770489	1400.216642	17.134119
36.269329	1405.864509	17.139136
36.382054	1430.664071	17.144154
36.350447	1429.184274	17.149171
36.693546	1414.816778	17.154189
36.347018	1406.681454	17.159207
36.385498	1390.871349	17.164224
36.383190	1396.441842	17.169242
36.560219	1407.100745	17.174259
36.706281	1410.788277	17.179277
36.574219	1394.934583	17.184295
36.396701	1389.163291	17.189312
36.420622	1395.412287	17.194330
36.882406	1404.540849	17.199347
36.960312	1409.832714	17.204365
36.811809	1398.068328	17.209383
36.643097	1383.853279	17.214400
36.706602	1390.143150	17.219418
36.855241	1400.949720	17.224435
36.912524	1408.093164	17.229453
36.653904	1412.516918	17.234471
37.050490	1405.298115	17.239488
37.124069	1408.572494	17.244506
37.247254	1402.828741	17.249523
36.823835	1388.709367	17.254541
36.869624	1391.220544	17.259559
37.000230	1398.728238	17.264576
36.965468	1406.927696	17.269594
36.718648	1410.621263	17.274611
37.316506	1402.204757	17.279629
37.149471	1414.843910	17.284647
37.521762	1408.915706	17.289664
37.265241	1404.034750	17.294682
37.115777	1405.974608	17.299699
37.603913	1407.024693	17.304717
37.042853	1416.500442	17.309735
37.132136	1393.531310	17.314752
37.246024	1414.122852	17.319770
37.453435	1408.147015	17.324787
37.564360	1403.830367	17.329805
37.164618	1415.076766	17.334823
37.510101	1394.649660	17.339840
37.644938	1401.873539	17.344858
37.462464	1406.058632	17.349875
37.482328	1400.081250	17.354893
37.902074	1416.567214	17.359911
37.729514	1417.979078	17.364928
37.744270	1417.292553	17.369946
37.936026	1416.664313	17.374963
37.883663	1403.763030	17.379981
37.663778	1421.760437	17.384999
37.944370	1427.389639	17.390016
38.326285	1420.357212	17.395034
37.912822	1422.993553	17.400051
38.389387	1402.386654	17.405069
38.198597	1404.471528	17.410087
38.081184	1408.065804	17.415104
37.987743	1401.060438	17.420122
37.972861	1402.409400	17.425139
38.050078	1398.949130	17.430157
38.353069	1430.658479	17.435175
38.121413	1435.869166	17.440192
38.628896	1428.434465	17.445210
38.223291	1419.163400	17.450227
38.589594	1421.088638	17.455245
38.414006	1407.489711	17.460263
38.207958	1394.723059	17.465280
38.298538	1410.209170	17.470298
38.275966	1424.436057	17.475315
38.397287	1428.866857	17.480333
38.387159	1434.037493	17.485351
38.342906	1430.893889	17.490368
38.497299	1425.635930	17.495386
38.355460	1428.268275	17.500403
38.691558	1444.113237	17.505421
38.730258	1438.993275	17.510439
38.673634	1428.873744	17.515456
38.745798	1428.168623	17.520474
38.605166	1438.771250	17.525491
39.136010	1432.690334	17.530509
38.938299	1452.609614	17.535527
39.076965	1450.358621	17.540544
39.183422	1440.565427	17.545562
39.049694	1424.782751	17.550579
38.970317	1444.236410	17.555597
38.791436	1442.975155	17.560615
39.296964	1449.529605	17.565632
39.393700	1445.893179	17.570650
38.904426	1461.726657	17.575667
39.369800	1456.854814	17.580685
39.116702	1456.580667	17.585703
39.104009	1452.164171	17.590720
39.394550	1463.545904	17.595738
39.184267	1451.069313	17.600755
39.428063	1443.862277	17.605773
39.393526	1445.595047	17.610791
39.374579	1450.653838	17.615808
39.535754	1444.921313	17.620826
39.134473	1447.466052	17.625843
39.468273	1447.198972	17.630861
39.466701	1460.228624	17.635879
39.275330	1455.842199	17.640896
39.944535	1459.377093	17.645914
39.861744	1470.528939	17.650931
40.005136	1456.219996	17.655949
39.827272	1452.190065	17.660967
40.059723	1452.376449	17.665984
40.123008	1441.853967	17.671002
39.840125	1449.959316	17.676019
39.931733	1444.292942	17.681037
39.712472	1451.541862	17.686055
39.820557	1455.207149	17.691072
40.283315	1466.553551	17.696090
39.946604	1476.600742	17.701107
40.299678	1476.528788	17.706125
40.383828	1480.938792	17.711143
39.926582	1472.736145	17.716160
39.894459	1476.936604	17.721178
39.971912	1480.468357	17.726195
40.448799	1482.655964	17.731213
40.225014	1473.486426	17.736231
40.334508	1473.791521	17.741248
40.502199	1474.110930	17.746266
40.218921	1474.239570	17.751283
40.255606	1478.298494	17.756301
40.549771	1469.494660	17.761319
40.599902	1465.429936	17.766336
40.605920	1464.510422	17.771354
40.398073	1476.511200	17.776371
40.812986	1480.736315	17.781389
41.036590	1473.505743	17.786407
40.753848	1474.046429	17.791424
40.754689	1478.520056	17.796442
40.719825	1479.523001	17.801459
40.630336	1480.001405	17.806477
40.727646	1490.193313	17.811495
41.070074	1491.557654	17.816512
41.167855	1478.989433	17.821530
40.708459	1494.862226	17.826547
41.483603	1498.355066	17.831565
41.413422	1485.500597	17.836583
40.905024	1497.226857	17.841600
41.486671	1485.227971	17.846618
41.352965	1486.556567	17.851635
41.622818	1488.871577	17.856653
41.594442	1487.392832	17.861671
41.555521	1484.743868	17.866688
41.542500	1468.575378	17.871706
41.156912	1464.482620	17.876723
41.615007	1466.976815	17.881741
41.412451	1474.633640	17.886759
41.315841	1483.450192	17.891776
41.627670	1484.633796	17.896794
41.587405	1485.245921	17.901811
41.835758	1488.289523	17.906829
42.007361	1487.582697	17.911847
41.525650	1477.244640	17.916864
41.682555	1475.534999	17.921882
41.749530	1487.595773	17.926899
41.905972	1487.811583	17.931917
42.205021	1476.513727	17.936935
41.634382	1485.775543	17.941952
41.828979	1478.401731	17.946970
41.842412	1487.068600	17.951987
41.992820	1482.954844	17.957005
41.860460	1489.593747	17.962023
41.669315	1487.308834	17.967040
42.117681	1470.250357	17.972058
41.995436	1488.510698	17.977075
41.598842	1482.717680	17.982093
41.998073	1482.537692	17.987111
42.077558	1501.365195	17.992128
42.411859	1502.800047	17.997146
42.233367	1518.090089	18.002163
42.359756	1518.521479	18.007181
42.594545	1513.947517	18.012199
42.173982	1515.071755	18.017216
42.565176	1512.371489	18.022234
42.271519	1520.871852	18.027251
42.396228	1520.174077	18.032269
42.780772	1506.727966	18.037287
42.883052	1509.392176	18.042304
42.696320	1512.668770	18.047322
42.824918	1502.404815	18.052339
42.869857	1522.131333	18.057357
42.920289	1506.588184	18.062375
42.736126	1507.196519	18.067392
43.212793	1495.035043	18.072410
43.052193	1511.385588	18.077427
43.018884	1508.808084	18.082445
43.176836	1498.165070	18.087463
42.850955	1502.816655	18.092480
42.967852	1505.382579	18.097498
43.061761	1501.131537	18.102515
43.073469	1501.389308	18.107533
43.024126	1510.855862	18.112551
43.085211	1526.941406	18.117568
43.242842	1532.709812	18.122586
43.330350	1535.708291	18.127603
43.494120	1530.950595	18.132621
43.712062	1528.630317	18.137639
43.637321	1533.707473	18.142656
43.491522	1533.757558	18.147674
43.547105	1530.008124	18.152691
43.847508	1525.238076	18.157709
43.846452	1531.360553	18.162727
43.518940	1520.107538	18.167744
44.022414	1527.352910	18.172762
43.796569	1533.542700	18.177779
43.773278	1537.833004	18.182797
43.834213	1523.524561	18.187815
43.679752	1537.923605	18.192832
43.921162	1522.095149	18.197850
43.774854	1526.590686	18.202867
43.801889	1529.348698	18.207885
43.964263	1534.056128	18.212903
43.717742	1527.477812	18.217920
44.032419	1530.477811	18.222938
44.079368	1532.461865	18.227955
43.945217	1518.536899	18.232973
44.013041	1526.861636	18.237991
44.015215	1532.991464	18.243008
44.225133	1537.931986	18.248026
44.323863	1561.900300	18.253043
44.125094	1563.813435	18.258061
44.613848	1552.943015	18.263079
44.539522	1554.940122	18.268096
44.677043	1558.108382	18.273114
44.608687	1546.159633	18.278131
44.547048	1552.208411	18.283149
44.486065	1559.710566	18.288167
44.485300	1559.268756	18.293184
44.638333	1551.182662	18.298202
44.746125	1543.048732	18.303219
44.689248	1551.679662	18.308237
45.022768	1545.732419	18.313255
44.475356	1555.305181	18.318272
44.834709	1551.864371	18.323290
44.919020	1551.133712	18.328307
44.797138	1551.691216	18.333325
45.089965	1560.853117	18.338343
45.147406	1568.989198	18.343360
45.264258	1580.200523	18.348378
45.381873	1574.331748	18.353395
45.376060	1570.515017	18.358413
45.350297	1565.076529	18.363431
44.896735	1568.414569	18.368448
45.560840	1573.595698	18.373466
45.463979	1570.539105	18.378483
45.106528	1569.119128	18.383501
45.358973	1572.097602	18.388519
45.816125	1569.918491	18.393536
45.738456	1572.079728	18.398554
45.889819	1573.875674	18.403571
45.807219	1578.608033	18.408589
45.814375	1568.615085	18.413607
45.785536	1575.187179	18.418624
45.910629	1577.586640	18.423642
46.194336	1576.073842	18.428659
45.578940	1583.302636	18.433677
46.037085	1575.944944	18.438695
45.906879	1567.064016	18.443712
45.789514	1565.676534	18.448730
45.697816	1581.744035	18.453747
45.769994	1577.350145	18.458765
45.532530	1568.067897	18.463783
45.414169	1574.312921	18.468800
45.750593	1584.792377	18.473818
46.017906	1603.218821	18.478835
46.011023	1609.597092	18.483853
46.049293	1613.706139	18.488871
46.137172	1607.571531	18.493888
46.476348	1607.759773	18.498906
46.491318	1607.974553	18.503923
46.615968	1607.372739	18.508941
46.549605	1609.552628	18.513959
46.515858	1606.412030	18.518976
46.432110	1600.635135	18.523994
46.750973	1599.752234	18.529011
46.672550	1604.281013	18.534029
46.735704	1598.861364	18.539047
47.126771	1611.073474	18.544064
47.071919	1614.185911	18.549082
47.065015	1593.646413	18.554099
47.036622	1605.667440	18.559117
47.170831	1604.057359	18.564135
47.235280	1601.575932	18.569152
46.904940	1606.843318	18.574170
47.137113	1605.019410	18.579187
46.909443	1600.492437	18.584205
47.184744	1601.919406	18.589223
46.848836	1611.947684	18.594240
47.009061	1617.467171	18.599258
47.041621	1614.304984	18.604275
47.164473	1622.551786	18.609293
47.415760	1617.492238	18.614311
47.400983	1618.680753	18.619328
47.492263	1630.668557	18.624346
47.453572	1621.543336	18.629363
47.211997	1619.710041	18.634381
47.222903	1613.834674	18.639399
47.673117	1635.651769	18.644416
47.842950	1641.314452	18.649434
47.892002	1638.887384	18.654451
48.086762	1638.631467	18.659469
48.317413	1632.991608	18.664487
47.922331	1615.079615	18.669504
47.711988	1624.721359	18.674522
48.324500	1621.123752	18.679539
47.817929	1630.041957	18.684557
48.219902	1626.960850	18.689575
48.356271	1639.229335	18.694592
48.575905	1640.482714	18.699610
48.558652	1607.450206	18.704627
48.318238	1612.429543	18.709645
48.405155	1599.180253	18.714663
48.460582	1606.693754	18.719680
48.113331	1614.306089	18.724698
48.642096	1594.283630	18.729715
48.141569	1607.515689	18.734733
48.362046	1607.493199	18.739751
48.677209	1617.123485	18.744768
48.613528	1633.612867	18.749786
48.542477	1628.194162	18.754803
48.565263	1637.391316	18.759821
48.704099	1627.548787	18.764839
48.814506	1624.031260	18.769856
48.652572	1642.394079	18.774874
48.881283	1623.772249	18.779891
49.027351	1639.720095	18.784909
48.705602	1633.188334	18.789927
48.865336	1623.531239	18.794944
48.818109	1632.237757	18.799962
49.286274	1634.215994	18.804979
49.164831	1625.527116	18.809997
49.003204	1632.400416	18.815015
49.149304	1627.475618	18.820032
49.123799	1624.094599	18.825050
49.343173	1635.544448	18.830067
49.568751	1657.194482	18.835085
49.559739	1643.523146	18.840103
49.721127	1641.159960	18.845120
49.557924	1635.721343	18.850138
49.532289	1620.287731	18.855155
49.365495	1636.213112	18.860173
49.307632	1647.560894	18.865191
49.642201	1652.292810	18.870208
49.758011	1651.613752	18.875226
49.840206	1651.646351	18.880243
49.355673	1656.562389	18.885261
49.334419	1650.416854	18.890279
49.562431	1654.903068	18.895296
49.722869	1683.377942	18.900314
50.071461	1675.438343	18.905331
50.189671	1685.825260	18.910349
50.292771	1677.456046	18.915367
50.450499	1669.616106	18.920384
50.213808	1675.073075	18.925402
50.741332	1675.317796	18.930419
50.513907	1676.535512	18.935437
50.529276	1674.922354	18.940455
50.788212	1655.831614	18.945472
50.565496	1651.140239	18.950490
50.676167	1639.875446	18.955507
50.564980	1642.594176	18.960525
50.865046	1635.908186	18.965543
50.859581	1630.337446	18.970560
50.616606	1636.740799	18.975578
50.789026	1632.363939	18.980595
50.701419	1634.880704	18.985613
50.071322	1641.076811	18.990631
50.736858	1646.580212	18.995648
50.794043	1671.030392	19.000666
50.866444	1669.977580	19.005683
51.199328	1671.143686	19.010701
51.140755	1671.316713	19.015719
51.333055	1668.668591	19.020736
51.065282	1668.544645	19.025754
51.183800	1656.414988	19.030771
51.195725	1677.169459	19.035789
51.226063	1673.700871	19.040807
51.185206	1658.055713	19.045824
51.303425	1664.755406	19.050842
51.547180	1662.544249	19.055859
51.389590	1659.621594	19.060877
51.176724	1664.502172	19.065895
51.707218	1666.377664	19.070912
51.148816	1676.634956	19.075930
51.711485	1664.058499	19.080947
51.803692	1684.446242	19.085965
51.688709	1697.815097	19.090983
51.766436	1693.593322	19.096000
51.562898	1699.040293	19.101018
51.801985	1681.852923	19.106035
51.843009	1686.691444	19.111053
51.647608	1684.709201	19.116071
52.050810	1676.108080	19.121088
51.893189	1696.505797	19.126106
52.086050	1704.035183	19.131123
52.607810	1705.674543	19.136141
52.203895	1703.576114	19.141159
52.470371	1707.365643	19.146176
52.742948	1708.037996	19.151194
52.882823	1694.176124	19.156211
52.664742	1686.130267	19.161229
52.165715	1678.693944	19.166247
52.837302	1667.695178	19.171264
52.288422	1688.016857	19.176282
52.184824	1700.059395	19.181299
52.605403	1704.332439	19.186317
52.608638	1713.752986	19.191335
52.668601	1709.497860	19.196352
52.451300	1717.419862	19.201370
52.479960	1711.593534	19.206387
52.911812	1713.486338	19.211405
52.896718	1724.954776	19.216423
53.282746	1732.580786	19.221440
53.371212	1736.589052	19.226458
53.464818	1727.909860	19.231475
53.219815	1699.402946	19.236493
53.171957	1702.939009	19.241511
53.473356	1712.618746	19.246528
53.348133	1729.250188	19.251546
53.502807	1734.618020	19.256563
53.537036	1733.827698	19.261581
53.530640	1737.017378	19.266599
53.647796	1724.505631	19.271616
53.324802	1734.542945	19.276634
53.484844	1730.551854	19.281651
53.553442	1727.914012	19.286669
53.330442	1734.668157	19.291687
53.557540	1735.651363	19.296704
53.618338	1732.580603	19.301722
53.447813	1721.077446	19.306739
53.973829	1730.977779	19.311757
53.842744	1750.364588	19.316775
54.374933	1737.438993	19.321792
54.429366	1755.037552	19.326810
54.072226	1754.334817	19.331827
54.693091	1727.102354	19.336845
54.077604	1736.857551	19.341863
54.213260	1735.516217	19.346880
54.290473	1750.449538	19.351898
54.307251	1749.152331	19.356915
54.698492	1755.010986	19.361933
54.471925	1762.267516	19.366951
55.021950	1754.171479	19.371968
54.460817	1751.394963	19.376986
54.424797	1743.120260	19.382003
54.665001	1740.173471	19.387021
54.912421	1745.893036	19.392039
54.923233	1752.410122	19.397056
54.794285	1744.059002	19.402074
55.023589	1744.153084	19.407091
55.140795	1743.816724	19.412109
54.751204	1743.278043	19.417127
55.125471	1745.456892	19.422144
55.170740	1751.216564	19.427162
55.455075	1747.558009	19.432179
55.154257	1737.463049	19.437197
55.276147	1753.306337	19.442215
55.418764	1746.319785	19.447232
55.353849	1745.073361	19.452250
55.190836	1735.659578	19.457267
55.546360	1738.063215	19.462285
55.291656	1754.875788	19.467303
55.444206	1763.464005	19.472320
55.876289	1763.796311	19.477338
55.328649	1774.871515	19.482355
55.715688	1769.950716	19.487373
55.591502	1770.308818	19.492391
55.684347	1775.033709	19.497408
55.814691	1770.718575	19.502426
55.561212	1762.398317	19.507443
55.713666	1768.682032	19.512461
55.675901	1778.975912	19.517479
56.192315	1787.512405	19.522496
56.263864	1793.879821	19.527514
56.001320	1795.617536	19.532531
56.430594	1781.833697	19.537549
56.579237	1798.794355	19.542567
56.861399	1781.280668	19.547584
56.865464	1794.345902	19.552602
56.467609	1785.494941	19.557619
56.524833	1776.816803	19.562637
56.537468	1792.822279	19.567655
57.079993	1781.401984	19.572672
57.310680	1770.830543	19.577690
56.800385	1768.189063	19.582707
56.785028	1756.780682	19.587725
56.601128	1756.961114	19.592743
56.816698	1760.717877	19.597760
56.714440	1769.500896	19.602778
56.969232	1786.107976	19.607795
57.169016	1774.583471	19.612813
57.046519	1778.505842	19.617831
56.864208	1786.077802	19.622848
57.194852	1782.084658	19.627866
57.038160	1785.141013	19.632883
57.463376	1771.386146	19.637901
57.223632	1767.974766	19.642919
57.252428	1775.418669	19.647936
57.425781	1776.992479	19.652954
57.681734	1794.293101	19.657971
57.815367	1793.571868	19.662989
57.647955	1816.544834	19.668007
57.644554	1804.170225	19.673024
57.492329	1802.907832	19.678042
57.520380	1809.030503	19.683059
57.729151	1798.591528	19.688077
57.269734	1813.185774	19.693095
57.558884	1809.587785	19.698112
57.753881	1820.019181	19.703130
58.058706	1830.648579	19.708147
58.423973	1840.352823	19.713165
58.290617	1838.675275	19.718183
58.305923	1828.583319	19.723200
58.732140	1831.693013	19.728218
58.277536	1843.889179	19.733235
58.587901	1830.201339	19.738253
58.431588	1829.005664	19.743271
58.330706	1829.577132	19.748288
58.589369	1830.523850	19.753306
58.588164	1823.396601	19.758323
58.698887	1824.313429	19.763341
58.826967	1833.232787	19.768359
58.426856	1827.790980	19.773376
59.163827	1817.003478	19.778394
58.947098	1838.743201	19.783411
58.985954	1835.845809	19.788429
58.863219	1837.676065	19.793447
59.396715	1846.074585	19.798464
59.533441	1849.246183	19.803482
59.002068	1847.901106	19.808499
59.356635	1852.996424	19.813517
59.498566	1854.405363	19.818535
59.546019	1848.283394	19.823552
59.476009	1851.078968	19.828570
59.110447	1861.889239	19.833587
59.405413	1854.385970	19.838605
59.487721	1853.029537	19.843623
59.610176	1855.772394	19.848640
59.678903	1850.493338	19.853658
59.518470	1861.662586	19.858675
59.657880	1853.416472	19.863693
59.719587	1844.072174	19.868711
59.574931	1852.163565	19.873728
60.160318	1844.423643	19.878746
60.380657	1874.040820	19.883763
60.240613	1861.667504	19.888781
60.081162	1854.197382	19.893799
60.314272	1852.214416	19.898816
60.588541	1860.147762	19.903834
59.934244	1860.061861	19.908851
60.088965	1854.344362	19.913869
60.396503	1879.247334	19.918887
60.280571	1884.243090	19.923904
60.657486	1872.633628	19.928922
60.310222	1870.416023	19.933939
60.754974	1868.728072	19.938957
60.811366	1887.039077	19.943975
60.631441	1881.187743	19.948992
60.792706	1874.132089	19.954010
60.643759	1883.822415	19.959027
61.049502	1888.563509	19.964045
61.108611	1889.282501	19.969063
61.056558	1902.846006	19.974080
61.348448	1898.783503	19.979098
61.284161	1894.131276	19.984115
61.487417	1893.282528	19.989133
61.470087	1898.338071	19.994151
61.430730	1900.015034	19.999168
61.537638	1894.464024	20.004186
61.469226	1889.936729	20.009203
61.473485	1896.583917	20.014221
61.558313	1884.059884	20.019239
61.268069	1890.999436	20.024256
61.497577	1896.927990	20.029274
61.502238	1901.739347	20.034291
61.592445	1890.867745	20.039309
61.736997	1895.659936	20.044327
62.044557	1914.410704	20.049344
62.325627	1915.720379	20.054362
62.048657	1936.846921	20.059379
62.328598	1921.491674	20.064397
62.446374	1921.526464	20.069415
62.061801	1926.827781	20.074432
62.458296	1924.762118	20.079450
62.245915	1915.404856	20.084467
62.469666	1921.482207	20.089485
62.274377	1919.304852	20.094503
62.441855	1915.089150	20.099520
62.914066	1906.110364	20.104538
62.518520	1924.359782	20.109555
62.648309	1922.119571	20.114573
62.678020	1918.378883	20.119591
62.612377	1918.230561	20.124608
62.994842	1910.472630	20.129626
62.718032	1911.754870	20.134643
62.771323	1906.588371	20.139661
63.157818	1925.801631	20.144679
63.277447	1935.282413	20.149696
63.380202	1934.802058	20.154714
63.085858	1940.597092	20.159731
63.209287	1929.617913	20.164749
63.385879	1937.321480	20.169767
62.994365	1935.983977	20.174784
63.033843	1940.722152	20.179802
63.122523	1940.739560	20.184819
63.437957	1926.739353	20.189837
63.503269	1942.563556	20.194855
63.749971	1957.972657	20.199872
64.156110	1954.777559	20.204890
63.805331	1960.321257	20.209907
63.915720	1954.400784	20.214925
64.121945	1958.859894	20.219943
64.047251	1956.497342	20.224960
64.163168	1954.452040	20.229978
64.197968	1955.251993	20.234995
64.180273	1946.157826	20.240013
64.198892	1948.199154	20.245031
64.532967	1959.861423	20.250048
64.785652	1951.507523	20.255066
64.536863	1953.205308	20.260083
64.552283	1949.067331	20.265101
64.637521	1950.626899	20.270119
64.102882	1959.099091	20.275136
64.559844	1948.732902	20.280154
64.386643	1949.836595	20.285171
64.533806	1964.154135	20.290189
64.885353	1973.848074	20.295207
64.998546	1974.705527	20.300224
65.174249	1970.282424	20.305242
65.178455	1975.784458	20.310259
64.939818	1981.701189	20.315277
65.106155	1971.867413	20.320295
65.167327	1975.589866	20.325312
65.428774	1967.438273	20.330330
65.484972	1965.219231	20.335347
65.333703	1963.719923	20.340365
65.589970	1959.741739	20.345383
65.170200	1979.153657	20.350400
65.436553	1991.746215	20.355418
65.556839	1995.334973	20.360435
65.813327	2002.048166	20.365453
66.335069	1995.222050	20.370471
65.843323	1998.725153	20.375488
66.228564	1996.577116	20.380506
66.389993	2002.757252	20.385523
66.240603	1984.933034	20.390541
66.088598	1991.897779	20.395559
65.900678	1990.797582	20.400576
66.430600	1987.505655	20.405594
66.249993	1994.926436	20.410611
66.073001	2006.671823	20.415629
65.971649	1996.920048	20.420647
66.375463	1993.582950	20.425664
66.626991	1999.238251	20.430682
66.186617	2004.535124	20.435699
66.130498	1999.754927	20.440717
66.254076	2011.832281	20.445735
66.265584	2022.196342	20.450752
66.616820	2017.667363	20.455770
66.700346	2031.623872	20.460787
67.086010	2041.089824	20.465805
67.507060	2042.270218	20.470823
67.712435	2046.801066	20.475840
67.374144	2026.058180	20.480858
67.527565	2016.198119	20.485875
67.251896	2027.986789	20.490893
67.577692	2017.902601	20.495911
67.032674	2023.706969	20.500928
67.469906	2032.221630	20.505946
67.552368	2044.116011	20.510963
67.298719	2050.720241	20.515981
67.669647	2045.761808	20.520999
67.722986	2052.776419	20.526016
67.534030	2056.918684	20.531034
67.634563	2050.009489	20.536051
67.817454	2046.953012	20.541069
68.279842	2049.210668	20.546087
67.997200	2074.013036	20.551104
68.466446	2069.556460	20.556122
68.639763	2071.206604	20.561139
68.532729	2068.835033	20.566157
68.730148	2048.669734	20.571175
68.551635	2049.237861	20.576192
68.321394	2047.323259	20.581210
68.505064	2054.114159	20.586227
68.681274	2064.857840	20.591245
68.605566	2060.352891	20.596263
68.549816	2070.938508	20.601280
68.856891	2063.495338	20.606298
69.093829	2070.437419	20.611315
68.842279	2076.306694	20.616333
69.103375	2053.995769	20.621351
69.449127	2066.362577	20.626368
69.554831	2058.971975	20.631386
69.246294	2059.296560	20.636403
69.340689	2060.464555	20.641421
69.374424	2060.429375	20.646439
69.092174	2065.032490	20.651456
69.332978	2056.316256	20.656474
69.621281	2047.915721	20.661491
69.224606	2060.494526	20.666509
69.410902	2049.832432	20.671527
69.315748	2074.790524	20.676544
69.407289	2087.632850	20.681562
69.902656	2097.512370	20.686579
69.737466	2084.018116	20.691597
70.243098	2089.373370	20.696615
69.883100	2089.258619	20.701632
69.997442	2089.607789	20.706650
70.210374	2086.369541	20.711667
70.069956	2081.896142	20.716685
70.178342	2096.170445	20.721703
70.334423	2115.362499	20.726720
70.416870	2104.005104	20.731738
70.738592	2107.455582	20.736755
70.456841	2114.973568	20.741773
70.754278	2111.115411	20.746791
70.571936	2112.580025	20.751808
70.590231	2107.761969	20.756826
70.902748	2098.207615	20.761843
70.558832	2105.577415	20.766861
70.956103	2119.525660	20.771879
70.869325	2125.665205	20.776896
71.085494	2138.352414	20.781914
71.239728	2137.067859	20.786931
71.573000	2143.849887	20.791949
71.592896	2128.029359	20.796967
71.675910	2132.966729	20.801984
71.698400	2136.494824	20.807002
71.884892	2126.764700	20.812019
71.821874	2133.658689	20.817037
71.631097	2122.174173	20.822055
71.709562	2129.102228	20.827072
71.614701	2134.010548	20.832090
71.710136	2120.128616	20.837107
71.803243	2118.348063	20.842125
71.910626	2119.442415	20.847143
71.976601	2126.918323	20.852160
72.012318	2133.683304	20.857178
72.519747	2146.130580	20.862195
72.075404	2152.510426	20.867213
72.539174	2150.247593	20.872231
72.764369	2159.064358	20.877248
72.801931	2150.783193	20.882266
72.546488	2136.810905	20.887283
72.636920	2142.760954	20.892301
72.708577	2144.077306	20.897319
72.995854	2154.395123	20.902336
72.915740	2155.336902	20.907354
72.970260	2145.864562	20.912371
72.771362	2149.132226	20.917389
72.949185	2152.538807	20.922407
72.957111	2138.928013	20.927424
72.966690	2144.866575	20.932442
73.109394	2140.226877	20.937459
72.873938	2167.029931	20.942477
73.212273	2169.822580	20.947495
73.359102	2177.310002	20.952512
73.260144	2174.948138	20.957530
73.771450	2163.151838	20.962547
73.443753	2174.115182	20.967565
73.663384	2163.186555	20.972583
74.105502	2169.233905	20.977600
73.637966	2181.341174	20.982618
73.620503	2173.119897	20.987635
73.502973	2190.320100	20.992653
74.145944	2199.565002	20.997671
73.934332	2197.589205	21.002688
73.765241	2208.375476	21.007706
74.312427	2192.450336	21.012723
74.328982	2223.348979	21.017741
74.760712	2218.185727	21.022759
75.072623	2230.392111	21.027776
74.923001	2203.100733	21.032794
74.992906	2185.021848	21.037811
74.820796	2193.027353	21.042829
74.911548	2188.694028	21.047847
74.954831	2192.572767	21.052864
74.919295	2208.058609	21.057882
75.145916	2201.244069	21.062899
75.323990	2216.529105	21.067917
75.279324	2215.217272	21.072935
75.447355	2212.637422	21.077952
75.342064	2213.742102	21.082970
75.371630	2209.000083	21.087987
75.077521	2218.075103	21.093005
75.308640	2210.572396	21.098023
75.661847	2204.317356	21.103040
75.410170	2217.710846	21.108058
75.578972	2215.189077	21.113075
75.977379	2221.314996	21.118093
76.076495	2238.615206	21.123111
75.988539	2247.759618	21.128128
75.972153	2248.931924	21.133146
76.153713	2239.333079	21.138163
75.988403	2244.386386	21.143181
75.942790	2246.958696	21.148199
76.132539	2239.655278	21.153216
76.289890	2241.007525	21.158234
76.344312	2248.838501	21.163251
76.730716	2269.478252	21.168269
76.760252	2268.457404	21.173287
77.007417	2272.177802	21.178304
76.960064	2277.387710	21.183322
77.236444	2263.797698	21.188339
76.990293	2265.138002	21.193357
77.161034	2260.906735	21.198375
77.475007	2257.746723	21.203392
76.829220	2263.015881	21.208410
77.348842	2260.693785	21.213427
77.372214	2267.788003	21.218445
77.384590	2254.785184	21.223463
77.223698	2255.591979	21.228480
77.507522	2256.454487	21.233498
77.547349	2266.796903	21.238515
77.706775	2266.232778	21.243533
77.604212	2258.301105	21.248551
77.893572	2254.452066	21.253568
77.590079	2256.907406	21.258586
77.958138	2257.564562	21.263603
77.957770	2266.322978	21.268621
77.860442	2268.836682	21.273639
78.099675	2277.227328	21.278656
77.976221	2277.669485	21.283674
78.388292	2279.030667	21.288691
78.093103	2281.154335	21.293709
78.382634	2279.498175	21.298727
78.244068	2274.657100	21.303744
78.304128	2289.873726	21.308762
78.596379	2293.899988	21.313779
78.901682	2292.854037	21.318797
79.053989	2303.079435	21.323815
78.945583	2306.448325	21.328832
78.802109	2305.366185	21.333850
78.998117	2303.287612	21.338867
78.726409	2305.363491	21.343885
78.714001	2310.309847	21.348903
79.161869	2318.698707	21.353920
79.315444	2336.805221	21.358938
79.192218	2320.970339	21.363955
79.318107	2313.637741	21.368973
79.594231	2329.850340	21.373991
79.944349	2330.743968	21.379008
79.768713	2330.605317	21.384026
80.126498	2335.812773	21.389043
80.182331	2348.860025	21.394061
80.262324	2354.706427	21.399079
80.107804	2323.798222	21.404096
80.123567	2344.872378	21.409114
80.313124	2348.895369	21.414131
80.302838	2357.977124	21.419149
80.073216	2350.193873	21.424167
80.598896	2354.639916	21.429184
80.445014	2346.044659	21.434202
80.628884	2351.333342	21.439219
80.566177	2354.075147	21.444237
80.473367	2349.740372	21.449255
80.836899	2354.819497	21.454272
80.718997	2373.799170	21.459290
81.183589	2366.661869	21.464307
81.632150	2374.013967	21.469325
81.482046	2386.648115	21.474343
81.556840	2374.642818	21.479360
81.622616	2371.401233	21.484378
81.568365	2368.680614	21.489395
81.505159	2366.050306	21.494413
81.292247	2363.575227	21.499431
81.597999	2359.407350	21.504448
81.711526	2363.457415	21.509466
81.448156	2370.043674	21.514483
81.457708	2367.448169	21.519501
81.522080	2370.008467	21.524519
81.798150	2363.028655	21.529536
81.734797	2390.027268	21.534554
82.098225	2392.818320	21.539571
82.103358	2405.494586	21.544589
81.936581	2401.730836	21.549607
82.677616	2391.110595	21.554624
82.157753	2402.815019	21.559642
82.358376	2402.328481	21.564659
82.604376	2416.407323	21.569677
82.181946	2428.741996	21.574695
82.732612	2407.597231	21.579712
82.868465	2418.254796	21.584730
82.851714	2424.878833	21.589747
83.025301	2422.473463	21.594765
82.772228	2420.807073	21.599783
83.450111	2428.685805	21.604800
83.399327	2441.540917	21.609818
83.407992	2446.414741	21.614835
83.524895	2445.351632	21.619853
83.518944	2447.864952	21.624871
83.833323	2437.986017	21.629888
83.861941	2440.809235	21.634906
84.154593	2441.795411	21.639923
84.237809	2443.987752	21.644941
83.970314	2434.763219	21.649959
84.453684	2437.174120	21.654976
84.262507	2442.195437	21.659994
84.072054	2428.964456	21.665011
84.524906	2435.957229	21.670029
84.081116	2436.536211	21.675047
84.380411	2432.359905	21.680064
84.219587	2435.501215	21.685082
84.133873	2432.663685	21.690099
84.529206	2450.837973	21.695117
84.434218	2458.377476	21.700135
84.869863	2442.431313	21.705152
84.917154	2454.945159	21.710170
85.104566	2462.228830	21.715187
85.077665	2458.501751	21.720205
84.575240	2474.401341	21.725223
85.047409	2465.606280	21.730240
85.337977	2484.458031	21.735258
85.337439	2484.896323	21.740275
85.597784	2478.475066	21.745293
85.569733	2487.516473	21.750311
85.603783	2475.983237	21.755328
85.773125	2481.241250	21.760346
85.702613	2476.198905	21.765363
85.831288	2476.906833	21.770381
85.779202	2478.255535	21.775399
85.995964	2475.379198	21.780416
86.127006	2489.654995	21.785434
86.772681	2496.123871	21.790451
86.903894	2495.439960	21.795469
86.389635	2490.049924	21.800487
86.577897	2480.119495	21.805504
86.773058	2475.666395	21.810522
86.348114	2495.466811	21.815539
86.540483	2494.018045	21.820557
86.447858	2500.424539	21.825575
86.748131	2504.576218	21.830592
86.964638	2505.764891	21.835610
86.851278	2501.928098	21.840627
87.281401	2506.613600	21.845645
86.985151	2504.187182	21.850663
86.872978	2521.832118	21.855680
87.164681	2530.393094	21.860698
87.475007	2537.695744	21.865715
87.660933	2533.757727	21.870733
87.628314	2548.496226	21.875751
87.481997	2529.650669	21.880768
87.565695	2538.468207	21.885786
87.651282	2543.198439	21.890803
88.106004	2553.502424	21.895821
88.074317	2565.602640	21.900839
88.111067	2553.654390	21.905856
88.662322	2547.583142	21.910874
88.661410	2554.715981	21.915891
88.717705	2548.689056	21.920909
88.609601	2544.237103	21.925927
88.585187	2545.317898	21.930944
88.939798	2550.468520	21.935962
88.704894	2550.663383	21.940979
89.023876	2538.729916	21.945997
88.920071	2538.792180	21.951015
88.775182	2543.512761	21.956032
88.982624	2551.089032	21.961050
88.974925	2555.025552	21.966067
89.376656	2559.854036	21.971085
89.294675	2575.861305	21.976103
89.510871	2570.176986	21.981120
89.667555	2583.592211	21.986138
89.426517	2588.178690	21.991155
89.747361	2574.651304	21.996173
89.494260	2580.358994	22.001191
89.533058	2580.013097	22.006208
90.136502	2590.453066	22.011226
89.688201	2602.738523	22.016243
90.087024	2598.497531	22.021261
90.198033	2603.923778	22.026279
90.224637	2598.772302	22.031296
90.577505	2594.318399	22.036314
90.133385	2600.267360	22.041331
90.649800	2588.179662	22.046349
90.200073	2596.497880	22.051367
90.680335	2614.681640	22.056384
90.912671	2622.530853	22.061402
91.189715	2615.332099	22.066419
91.496945	2624.888816	22.071437
91.267800	2621.252154	22.076455
91.077501	2623.702088	22.081472
91.518039	2623.656307	22.086490
91.090128	2633.224863	22.091507
91.795991	2614.706588	22.096525
91.387887	2623.671038	22.101543
91.433806	2621.113737	22.106560
91.685694	2606.692760	22.111578
91.775478	2617.322423	22.116595
91.609158	2612.846697	22.121613
91.683522	2622.332787	22.126631
91.883777	2629.778102	22.131648
92.304877	2622.428161	22.136666
92.243818	2642.269068	22.141683
92.379434	2630.019462	22.146701
92.474826	2628.476028	22.151719
92.126292	2639.080431	22.156736
92.180157	2633.062510	22.161754
92.095363	2636.175220	22.166771
92.441841	2658.565728	22.171789
92.403348	2667.497219	22.176807
92.658131	2665.847346	22.181824
93.114327	2669.044477	22.186842
92.662468	2689.156997	22.191859
93.127232	2691.625971	22.196877
93.418793	2693.070913	22.201895
93.131323	2699.377208	22.206912
93.398820	2693.171026	22.211930
93.636010	2696.123854	22.216947
93.336151	2699.143448	22.221965
93.615477	2715.452717	22.226983
93.810946	2719.125629	22.232000
94.613644	2702.179903	22.237018
93.957260	2727.053205	22.242035
94.268061	2718.957825	22.247053
94.391346	2709.463928	22.252071
94.145184	2721.800627	22.257088
94.518714	2715.465045	22.262106
94.414223	2725.137040	22.267123
94.944279	2704.661366	22.272141
94.696922	2713.904641	22.277159
94.417440	2715.456382	22.282176
95.011044	2712.655983	22.287194
94.584837	2740.456425	22.292211
95.431152	2727.278507	22.297229
95.474824	2731.805469	22.302247
95.273711	2723.672162	22.307264
95.646074	2732.589301	22.312282
95.341685	2737.564273	22.317299
95.271937	2725.228564	22.322317
95.432897	2724.825428	22.327335
95.495090	2731.923907	22.332352
95.465371	2726.333804	22.337370
95.533028	2727.605226	22.342387
95.887818	2747.217925	22.347405
96.260035	2740.429473	22.352423
96.148641	2755.656623	22.357440
96.140631	2756.387936	22.362458
96.372806	2751.017204	22.367475
96.429783	2743.961244	22.372493
96.471552	2755.048588	22.377511
96.363278	2744.716918	22.382528
96.774259	2755.171182	22.387546
96.762598	2762.658225	22.392563
96.956497	2751.562575	22.397581
96.877712	2767.623032	22.402599
96.790869	2781.188183	22.407616
97.069977	2770.880457	22.412634
97.405621	2785.197854	22.417651
97.321975	2775.537909	22.422669
97.631440	2773.154077	22.427687
97.716728	2789.376385	22.432704
98.171320	2764.395325	22.437722
97.751697	2782.204445	22.442739
97.635928	2773.424302	22.447757
98.217173	2763.637884	22.452775
97.810169	2777.033057	22.457792
97.713933	2792.574821	22.462810
97.923098	2807.367055	22.467827
97.920312	2801.407654	22.472845
98.035267	2802.090256	22.477863
98.032837	2812.747353	22.482880
98.395538	2826.513015	22.487898
98.549345	2835.727790	22.492915
98.426608	2830.150907	22.497933
98.682862	2818.938288	22.502951
98.807831	2841.211804	22.507968
99.173748	2853.782945	22.512986
99.064372	2863.499072	22.518003
98.986958	2860.325049	22.523021
98.991872	2862.305763	22.528039
99.152926	2864.218316	22.533056
99.559876	2862.412010	22.538074
99.613493	2883.731829	22.543091
99.751332	2885.282324	22.548109
99.896870	2875.165728	22.553127
99.798536	2874.277711	22.558144
100.103530	2878.676522	22.563162
99.975334	2876.467869	22.568179
99.967669	2870.549334	22.573197
100.633505	2882.113823	22.578215
100.237713	2895.665421	22.583232
100.642081	2895.324934	22.588250
100.864317	2900.123163	22.593267
101.322693	2896.384659	22.598285
101.237439	2879.353007	22.603303
100.819090	2873.159370	22.608320
101.148376	2872.618479	22.613338
101.131962	2883.630247	22.618355
101.297682	2885.829164	22.623373
101.545134	2892.862782	22.628391
101.199627	2893.943678	22.633408
101.373135	2886.791980	22.638426
101.397047	2888.173436	22.643443
101.201135	2896.655072	22.648461
101.527232	2891.142671	22.653479
101.493401	2905.261106	22.658496
101.930432	2910.583564	22.663514
102.109760	2911.772694	22.668531
102.282770	2912.730003	22.673549
102.510304	2907.053971	22.678567
102.366273	2920.256315	22.683584
102.565257	2918.623965	22.688602
102.654864	2923.405596	22.693619
102.495377	2928.163237	22.698637
102.722119	2916.335417	22.703655
102.513332	2936.968778	22.708672
102.767604	2939.799372	22.713690
102.906375	2950.970506	22.718707
103.337265	2953.349752	22.723725
103.188776	2954.923890	22.728743
102.979840	2956.174153	22.733760
103.171963	2956.359918	22.738778
103.740399	2968.469385	22.743795
103.647886	2982.041919	22.748813
104.003686	2978.101866	22.753831
103.987393	2977.901613	22.758848
104.063783	2976.976288	22.763866
103.913999	2976.832718	22.768883
103.901563	2968.338030	22.773901
104.344589	2981.746505	22.778919
104.403445	3004.936181	22.783936
104.371608	3001.328526	22.788954
104.456753	2998.166306	22.793971
104.473293	3004.591795	22.798989
105.161640	3000.465773	22.804007
105.131734	3011.088066	22.809024
104.813807	3001.002814	22.814042
105.046135	2995.422735	22.819059
105.229947	3003.305064	22.824077
105.526640	3019.074662	22.829095
105.354967	3021.458763	22.834112
105.398029	3015.884474	22.839130
105.591447	3012.889049	22.844147
105.581305	3019.299921	22.849165
105.802210	3010.196145	22.854183
105.813585	3008.515830	22.859200
106.018275	3014.177429	22.864218
105.858556	3003.348786	22.869235
105.989158	3026.903048	22.874253
106.484714	3025.681192	22.879271
106.254403	3043.378633	22.884288
106.567231	3040.833758	22.889306
106.750845	3030.636256	22.894323
106.327368	3032.185032	22.899341
106.350258	3036.342558	22.904359
106.651253	3048.049527	22.909376
106.899462	3038.019490	22.914394
107.173556	3059.850305	22.919411
107.145297	3060.622619	22.924429
107.312984	3057.402388	22.929447
107.189855	3065.887460	22.934464
106.942192	3065.755565	22.939482
107.514784	3082.623375	22.944499
107.526724	3086.213950	22.949517
107.652193	3096.715564	22.954535
107.782929	3085.754803	22.959552
107.875218	3097.507679	22.964570
108.001954	3112.217402	22.969587
108.146645	3118.104137	22.974605
108.409427	3115.411483	22.979623
108.491493	3112.017683	22.984640
108.259775	3120.811932	22.989658
108.705991	3115.927665	22.994675
108.609307	3146.843964	22.999693
109.006050	3138.488444	23.004711
108.867209	3140.140509	23.009728
109.317231	3133.170352	23.014746
109.378426	3129.535244	23.019763
109.372310	3133.522797	23.024781
109.785874	3136.450738	23.029799
109.338596	3126.251516	23.034816
109.401166	3135.240331	23.039834
109.849654	3150.206346	23.044851
109.963913	3156.860952	23.049869
109.952934	3164.540810	23.054887
109.931033	3161.806231	23.059904
110.048307	3155.314677	23.064922
110.187129	3146.813070	23.069939
110.164152	3173.895580	23.074957
110.084005	3178.529739	23.079975
110.682958	3183.665224	23.084992
110.501485	3183.728863	23.090010
111.091809	3178.655622	23.095027
110.823408	3181.748170	23.100045
111.223472	3189.204387	23.105063
111.301226	3200.925840	23.110080
111.441572	3207.273467	23.115098
111.675123	3208.437458	23.120115
111.742040	3214.518340	23.125133
112.016566	3196.492886	23.130151
112.086900	3213.330029	23.135168
111.884368	3206.080820	23.140186
112.431227	3194.565928	23.145203
112.196379	3199.513445	23.150221
112.233947	3190.011668	23.155239
112.660060	3176.390643	23.160256
112.752914	3183.616602	23.165274
112.884894	3174.456111	23.170291
112.076056	3165.466102	23.175309
112.845106	3176.385877	23.180327
112.943018	3178.400574	23.185344
112.357334	3194.058570	23.190362
112.629367	3187.166326	23.195379
112.790614	3190.036975	23.200397
112.575733	3202.721487	23.205415
112.802554	3228.792023	23.210432
112.671833	3216.909266	23.215450
113.128852	3242.250907	23.220467
113.294467	3256.886928	23.225485
113.752185	3245.632419	23.230503
113.761670	3260.298060	23.235520
113.503787	3268.279284	23.240538
114.066338	3267.314961	23.245555
114.185015	3285.665777	23.250573
114.187502	3279.068187	23.255591
114.101179	3278.349710	23.260608
114.464000	3284.648522	23.265626
114.461994	3297.115890	23.270643
114.666273	3309.548801	23.275661
114.747989	3309.141768	23.280679
115.146253	3299.735792	23.285696
115.372100	3306.455267	23.290714
115.536376	3304.740310	23.295731
115.352552	3308.356651	23.300749
115.470233	3303.706419	23.305767
115.803556	3306.908345	23.310784
115.826752	3320.408466	23.315802
115.509410	3324.103524	23.320819
115.814136	3347.348931	23.325837
116.063771	3319.253165	23.330855
116.244858	3312.903181	23.335872
115.988477	3327.180223	23.340890
116.370525	3328.868026	23.345907
116.546972	3333.226120	23.350925
116.483728	3346.559914	23.355943
116.855688	3347.602733	23.360960
116.926841	3347.268965	23.365978
117.139683	3354.088076	23.370995
117.010029	3358.964597	23.376013
117.130307	3346.704252	23.381031
117.223561	3339.849099	23.386048
116.922636	3354.206425	23.391066
117.317302	3364.968151	23.396083
117.618984	3373.223618	23.401101
117.822928	3370.239029	23.406119
117.922729	3369.396473	23.411136
118.210008	3371.287394	23.416154
118.141651	3369.080135	23.421171
118.086904	3369.537324	23.426189
118.395651	3374.443842	23.431207
118.481650	3360.197248	23.436224
118.457493	3368.232503	23.441242
118.758833	3370.881836	23.446259
118.977527	3382.319805	23.451277
118.704494	3389.953467	23.456295
118.980962	3387.391520	23.461312
119.251032	3390.847403	23.466330
119.255025	3388.096853	23.471347
119.191937	3391.387182	23.476365
119.122035	3385.391835	23.481383
119.672173	3371.406316	23.486400
119.264512	3402.855726	23.491418
119.521902	3405.914033	23.496435
119.491164	3415.341098	23.501453
119.715836	3409.144592	23.506471
119.899687	3423.128130	23.511488
119.877002	3438.737512	23.516506
120.156345	3441.627924	23.521523
120.089586	3448.029134	23.526541
120.426980	3452.433968	23.531559
120.925464	3454.214133	23.536576
120.825590	3477.696535	23.541594
120.944173	3481.492029	23.546611
121.286879	3474.174621	23.551629
121.081806	3467.077504	23.556647
121.192604	3470.411705	23.561664
121.087389	3471.346556	23.566682
121.566232	3474.698372	23.571699
121.675848	3490.855439	23.576717
121.536553	3495.624988	23.581735
121.943054	3498.283534	23.586752
121.985383	3492.602201	23.591770
121.834852	3493.559224	23.596787
122.100091	3519.051494	23.601805
122.300341	3521.674497	23.606823
122.447434	3526.398390	23.611840
122.434275	3528.800559	23.616858
122.706897	3518.595605	23.621875
122.766037	3532.791856	23.626893
122.757241	3548.194619	23.631911
123.401998	3536.722061	23.636928
123.224366	3549.323056	23.641946
123.332515	3544.417829	23.646963
123.630934	3541.705258	23.651981
123.787515	3541.859729	23.656999
124.054619	3536.343124	23.662016
124.062073	3544.282974	23.667034
124.509173	3550.397767	23.672051
124.091606	3544.131345	23.677069
124.600630	3556.927277	23.682087
124.695376	3541.688754	23.687104
124.697951	3548.441584	23.692122
124.795848	3541.912044	23.697139
124.794041	3530.791163	23.702157
124.460447	3539.467394	23.707175
124.872477	3558.273640	23.712192
124.759554	3565.979404	23.717210
124.806266	3543.852213	23.722227
125.122483	3552.173901	23.727245
124.878377	3577.242481	23.732263
125.293256	3574.575836	23.737280
125.332479	3604.243511	23.742298
125.020923	3586.878977	23.747315
125.580719	3587.714873	23.752333
125.639888	3616.577822	23.757351
125.761316	3608.715102	23.762368
125.884851	3628.301363	23.767386
125.845110	3639.112111	23.772403
126.289751	3631.802757	23.777421
125.945402	3648.188925	23.782439
126.277694	3667.702619	23.787456
126.710323	3673.692339	23.792474
126.978561	3673.821928	23.797491
126.978174	3662.998852	23.802509
126.952259	3679.825135	23.807527
127.548160	3690.929452	23.812544
127.747407	3693.859432	23.817562
127.608914	3688.825147	23.822579
128.232460	3698.494181	23.827597
127.851415	3683.448587	23.832615
128.098181	3689.147793	23.837632
128.256696	3686.381987	23.842650
128.366028	3679.690877	23.847667
128.196467	3691.084804	23.852685
128.404041	3707.139961	23.857703
128.606475	3717.500742	23.862720
128.828533	3723.867818	23.867738
128.661588	3709.234078	23.872755
128.904595	3715.729177	23.877773
128.734494	3729.166888	23.882791
129.265951	3728.838377	23.887808
129.532385	3740.287108	23.892826
129.491683	3739.068113	23.897843
130.013749	3734.587681	23.902861
129.888933	3727.212543	23.907879
130.126052	3732.825201	23.912896
130.152422	3728.039149	23.917914
129.884750	3740.998424	23.922931
130.046206	3755.842494	23.927949
130.420865	3762.659594	23.932967
130.773657	3759.710976	23.937984
130.917187	3768.621194	23.943002
130.955220	3769.452985	23.948019
130.834781	3762.798475	23.953037
131.110755	3773.281297	23.958055
131.399844	3767.571523	23.963072
130.959361	3772.702268	23.968090
131.268882	3780.159857	23.973107
131.453335	3777.322248	23.978125
131.679182	3776.729388	23.983143
131.736283	3770.734870	23.988160
131.811326	3774.325779	23.993178
132.020436	3775.805223	23.998195
132.226422	3777.114466	24.003213
131.904655	3798.485251	24.008231
132.349505	3792.116602	24.013248
132.501826	3799.968199	24.018266
132.534929	3804.593937	24.023283
132.528428	3794.455326	24.028301
132.763443	3821.649718	24.033319
132.873887	3823.084328	24.038336
133.003528	3828.528515	24.043354
132.893132	3825.040952	24.048371
133.605321	3835.274123	24.053389
133.694207	3855.891990	24.058407
133.795933	3848.472801	24.063424
133.930414	3849.037493	24.068442
134.339544	3848.995944	24.073459
134.706313	3842.045812	24.078477
134.357859	3849.909636	24.083495
134.168986	3851.329046	24.088512
134.324732	3846.639534	24.093530
134.273645	3848.895982	24.098547
134.559715	3867.383672	24.103565
134.275721	3875.640778	24.108583
134.799475	3868.631776	24.113600
134.738558	3882.104922	24.118618
134.697218	3903.913355	24.123635
134.946417	3891.237105	24.128653
135.187494	3916.609634	24.133671
135.773645	3932.739190	24.138688
135.862054	3933.242006	24.143706
135.760455	3934.807983	24.148723
136.275170	3932.923013	24.153741
136.203067	3954.763174	24.158759
136.628076	3957.640690	24.163776
136.687042	3957.402464	24.168794
136.594363	3966.289895	24.173811
137.131355	3947.818122	24.178829
137.060787	3956.299260	24.183847
137.062077	3950.289969	24.188864
137.170461	3956.078210	24.193882
137.420523	3964.166037	24.198899
137.483846	3976.939012	24.203917
137.400407	3979.181759	24.208935
137.701297	3982.579378	24.213952
137.619445	3987.317900	24.218970
137.288050	3991.386660	24.223987
137.895845	4005.381821	24.229005
138.227806	4011.961200	24.234023
138.272072	4013.158588	24.239040
138.680257	3999.860616	24.244058
138.410661	4018.160199	24.249075
138.765905	4018.882425	24.254093
138.654193	4035.768422	24.259111
139.108380	4028.771225	24.264128
139.211140	4030.825387	24.269146
139.035613	4043.883513	24.274163
139.343358	4031.997829	24.279181
139.543885	4051.403251	24.284199
139.641933	4061.821827	24.289216
139.726516	4063.223613	24.294234
140.175159	4058.504638	24.299251
140.448772	4055.433285	24.304269
140.105224	4065.646950	24.309287
140.356366	4058.623116	24.314304
140.644429	4060.626496	24.319322
140.236906	4075.835370	24.324339
140.509036	4086.044490	24.329357
140.552127	4091.475830	24.334375
140.619412	4092.118898	24.339392
141.102332	4102.888341	24.344410
140.923713	4104.693172	24.349427
141.281107	4113.201346	24.354445
141.410529	4144.732686	24.359463
141.845011	4136.961366	24.364480
141.987330	4137.919720	24.369498
141.762904	4142.931182	24.374515
142.326782	4143.819958	24.379533
142.528141	4159.521036	24.384551
142.574302	4162.752425	24.389568
142.849365	4167.300364	24.394586
142.996088	4168.942408	24.399603
143.211081	4157.858068	24.404621
143.351542	4160.408910	24.409639
143.217350	4161.089613	24.414656
143.367972	4153.147216	24.419674
143.363132	4168.684518	24.424691
143.436127	4163.130980	24.429709
143.782338	4170.206899	24.434727
143.798909	4188.852033	24.439744
143.825172	4175.650987	24.444762
143.859518	4193.107801	24.449779
144.288517	4203.461909	24.454797
144.124703	4217.151579	24.459815
144.180782	4218.840336	24.464832
145.085749	4231.286601	24.469850
144.823476	4240.922606	24.474867
145.110345	4236.170371	24.479885
145.498319	4233.913032	24.484903
145.520685	4240.101351	24.489920
145.644206	4230.320877	24.494938
145.553662	4234.738334	24.499955
145.730392	4237.503672	24.504973
145.589788	4258.928050	24.509991
145.738767	4264.513276	24.515008
146.194240	4256.830586	24.520026
145.889602	4269.359622	24.525043
146.008625	4274.976374	24.530061
146.368643	4285.660137	24.535079
146.325815	4291.331809	24.540096
146.544534	4288.094522	24.545114
146.642490	4298.662748	24.550131
146.790806	4319.964055	24.555149
146.789464	4325.297939	24.560167
147.076198	4329.336670	24.565184
147.671490	4337.828284	24.570202
147.838498	4349.198947	24.575219
148.111577	4346.961485	24.580237
148.137635	4346.331234	24.585255
147.855507	4345.587283	24.590272
148.260596	4344.380544	24.595290
148.128400	4367.771976	24.600307
148.591262	4372.199569	24.605325
148.676698	4372.317409	24.610343
148.882518	4376.372201	24.615360
149.157107	4368.172348	24.620378
149.274282	4380.270781	24.625395
149.547209	4391.753603	24.630413
149.640609	4389.614010	24.635431
149.663665	4393.531175	24.640448
149.960181	4388.889060	24.645466
149.928493	4396.070185	24.650483
150.066042	4387.107078	24.655501
150.108927	4407.564709	24.660519
150.096202	4417.886348	24.665536
150.375883	4425.268000	24.670554
150.131705	4428.312100	24.675571
150.240381	4438.578210	24.680589
150.736615	4437.811626	24.685607
151.028199	4452.905484	24.690624
151.338135	4461.033601	24.695642
151.334429	4477.304227	24.700659
151.544213	4469.229506	24.705677
151.858966	4485.998461	24.710695
151.490606	4481.046967	24.715712
152.180098	4486.596441	24.720730
152.259331	4501.020135	24.725747
152.528973	4500.327438	24.730765
152.839582	4491.505023	24.735783
152.742429	4507.154950	24.740800
152.809877	4487.946310	24.745818
152.869282	4496.862519	24.750835
153.289144	4499.040829	24.755853
153.132253	4507.127765	24.760871
153.311672	4522.996359	24.765888
153.765326	4516.885602	24.770906
153.478891	4532.455601	24.775923
153.582744	4523.063540	24.780941
154.058081	4520.878764	24.785959
153.913467	4547.139891	24.790976
154.196787	4547.794948	24.795994
154.251774	4552.372592	24.801011
154.399924	4554.323616	24.806029
154.423156	4540.814349	24.811047
154.460371	4566.189041	24.816064
155.048675	4566.929992	24.821082
155.021963	4570.247038	24.826099
155.056126	4570.823035	24.831117
155.684066	4566.682628	24.836135
155.522062	4578.834393	24.841152
155.894555	4586.595454	24.846170
155.935956	4593.369322	24.851187
156.069751	4593.780752	24.856205
156.107461	4593.886537	24.861223
155.980191	4592.641153	24.866240
156.557782	4610.851232	24.871258
156.628289	4618.886238	24.876275
156.460525	4626.277975	24.881293
156.651989	4623.904803	24.886311
156.619051	4636.654366	24.891328
157.111515	4648.992909	24.896346
157.049079	4650.042159	24.901363
157.422595	4655.033190	24.906381
157.593704	4672.469554	24.911399
157.397667	4690.821964	24.916416
157.671387	4693.774889	24.921434
157.792737	4699.559784	24.926451
158.002330	4712.631044	24.931469
158.002769	4723.847619	24.936487
158.223121	4743.911613	24.941504
158.493186	4735.241841	24.946522
158.715060	4759.130482	24.951539
158.974075	4768.428827	24.956557
159.584846	4774.392963	24.961575
159.623909	4771.225912	24.966592
159.930961	4749.428285	24.971610
160.013692	4751.203323	24.976627
159.825177	4759.379614	24.981645
160.272157	4771.996920	24.986663
160.280396	4781.203095	24.991680
160.955467	4790.284860	24.996698
160.872267	4790.915766	25.001715
160.881718	4783.574542	25.006733
161.303682	4771.574077	25.011751
161.032223	4795.079649	25.016768
161.003330	4780.856291	25.021786
161.365770	4796.517422	25.026803
161.387383	4807.529293	25.031821
161.583239	4813.225258	25.036839
161.800196	4818.826604	25.041856
162.390671	4824.911215	25.046874
162.611036	4830.255562	25.051891
162.490232	4837.594288	25.056909
162.850444	4838.246540	25.061927
162.778213	4829.610835	25.066944
162.791522	4832.363008	25.071962
162.917043	4825.705772	25.076979
162.828764	4842.612559	25.081997
162.718415	4845.142936	25.087015
162.724779	4862.095231	25.092032
163.101696	4858.281126	25.097050
162.893167	4879.611034	25.102067
163.346883	4889.393698	25.107085
163.683015	4894.658247	25.112103
163.903940	4911.416690	25.117120
164.166942	4924.500078	25.122138
164.587738	4925.318108	25.127155
164.480992	4926.065271	25.132173
164.647650	4939.226182	25.137191
165.018467	4958.150157	25.142208
165.049028	4954.378664	25.147226
165.176473	4950.939446	25.152243
165.343538	4973.293673	25.157261
165.702785	4976.646823	25.162279
165.662024	4990.212960	25.167296
165.755513	4984.277443	25.172314
166.018987	5006.458223	25.177331
165.928267	5007.443565	25.182349
166.089183	5012.143708	25.187367
166.003794	5029.572618	25.192384
166.364350	5026.040359	25.197402
166.796876	5042.200361	25.202419
166.787705	5059.396877	25.207437
167.427247	5062.285257	25.212455
167.410378	5061.720036	25.217472
167.879038	5053.789384	25.222490
168.058277	5074.868152	25.227507
168.080460	5086.244384	25.232525
168.144164	5075.170892	25.237543
168.345374	5078.901707	25.242560
168.430359	5079.722940	25.247578
168.578688	5088.785031	25.252595
168.594414	5102.588504	25.257613
169.012100	5110.592813	25.262631
168.711923	5121.188134	25.267648
169.071864	5127.182970	25.272666
169.427143	5134.110799	25.277683
169.210447	5145.730495	25.282701
169.571801	5144.680931	25.287719
169.809368	5161.990062	25.292736
170.290355	5159.916010	25.297754
170.423476	5155.242280	25.302771
170.445810	5163.937446	25.307789
171.147260	5173.594265	25.312807
171.108891	5185.985643	25.317824
170.952480	5190.861525	25.322842
171.417480	5186.042827	25.327859
171.477311	5184.518173	25.332877
171.704506	5186.894092	25.337895
171.687506	5192.657184	25.342912
171.942047	5197.738962	25.347930
171.939787	5192.203330	25.352947
171.753697	5208.940467	25.357965
171.936740	5215.683385	25.362983
171.838489	5220.715214	25.368000
172.144058	5234.312108	25.373018
172.596788	5245.638699	25.378035
172.632832	5256.859444	25.383053
172.876970	5262.993954	25.388071
172.887721	5276.979327	25.393088
173.101755	5280.908761	25.398106
173.348565	5289.127651	25.403123
173.668800	5314.839280	25.408141
173.893318	5316.372287	25.413159
174.062158	5305.402227	25.418176
173.950193	5326.307504	25.423194
174.577046	5334.987420	25.428211
174.879101	5344.109339	25.433229
174.826605	5332.536519	25.438247
174.829018	5354.252013	25.443264
175.346199	5363.579595	25.448282
175.785378	5346.410323	25.453299
175.341583	5360.008803	25.458317
175.919454	5350.955241	25.463335
176.381070	5357.421727	25.468352
175.909036	5364.757709	25.473370
175.889873	5379.927242	25.478387
176.336094	5388.875153	25.483405
176.309775	5392.816978	25.488423
176.478102	5407.151830	25.493440
176.675140	5413.544090	25.498458
177.101711	5408.128032	25.503475
176.619300	5425.052695	25.508493
176.971836	5445.977703	25.513511
177.299275	5450.980288	25.518528
177.111040	5466.050990	25.523546
177.740821	5473.998082	25.528563
178.003355	5480.476696	25.533581
178.190731	5492.928320	25.538599
178.155781	5502.589478	25.543616
178.294231	5511.924827	25.548634
178.644912	5524.632877	25.553651
179.051997	5530.356809	25.558669
179.563766	5518.481463	25.563687
179.339719	5538.762154	25.568704
179.844164	5557.605019	25.573722
179.984043	5562.324428	25.578739
180.201106	5564.134793	25.583757
180.009865	5558.005276	25.588775
180.044551	5556.571920	25.593792
180.306776	5570.884095	25.598810
181.021524	5567.830216	25.603827
180.752105	5574.697362	25.608845
181.119980	5576.078517	25.613863
181.053081	5576.515680	25.618880
181.102403	5595.825309	25.623898
181.404627	5598.582699	25.628915
181.618598	5600.176423	25.633933
181.712635	5605.689101	25.638951
181.818400	5617.956373	25.643968
182.135558	5626.292474	25.648986
182.509047	5626.530402	25.654003
182.612768	5634.538639	25.659021
182.787319	5635.776754	25.664039
183.187134	5650.085164	25.669056
182.869632	5658.677456	25.674074
183.112539	5663.028015	25.679092
183.545142	5663.217968	25.684109
183.412247	5661.871113	25.689127
183.559293	5685.165828	25.694144
183.699967	5692.365734	25.699162
183.908010	5684.553400	25.704180
184.141335	5715.687615	25.709197
184.272537	5722.525573	25.714215
184.462570	5713.799544	25.719232
184.349534	5737.540978	25.724250
184.990320	5744.808296	25.729268
185.289680	5753.145733	25.734285
185.537228	5773.770890	25.739303
185.693033	5769.083123	25.744320
185.736091	5778.267848	25.749338
186.293993	5765.204052	25.754356
186.350020	5771.904537	25.759373
186.753613	5778.052391	25.764391
186.966074	5777.042261	25.769408
186.759671	5796.322116	25.774426
187.282381	5789.987413	25.779444
187.201536	5790.703740	25.784461
186.686783	5795.263248	25.789479
187.548760	5799.725995	25.794496
187.530572	5818.321301	25.799514
187.784573	5819.365815	25.804532
187.928090	5846.790967	25.809549
187.784195	5851.066357	25.814567
188.419028	5851.436494	25.819584
188.366912	5874.840363	25.824602
188.815152	5886.927378	25.829620
188.821557	5880.523897	25.834637
189.254469	5888.859002	25.839655
189.330369	5896.108672	25.844672
189.448571	5909.162525	25.849690
189.670173	5912.703844	25.854708
189.866591	5926.197622	25.859725
189.890136	5934.291186	25.864743
190.489312	5933.522291	25.869760
190.501322	5946.829919	25.874778
190.681390	5953.216466	25.879796
190.907887	5955.475398	25.884813
190.977976	5965.399408	25.889831
190.959116	5964.165731	25.894848
190.871008	5974.656254	25.899866
191.381328	5977.310521	25.904884
191.650971	5981.643537	25.909901
191.698954	5999.311168	25.914919
192.161277	6004.792816	25.919936
192.371208	6021.119201	25.924954
192.520924	6013.407258	25.929972
192.343174	6015.013128	25.934989
193.087144	6041.364190	25.940007
193.474998	6038.280516	25.945024
193.180655	6050.987219	25.950042
193.320903	6039.228126	25.955060
193.827041	6050.686083	25.960077
193.784571	6068.056661	25.965095
194.054373	6063.573280	25.970112
193.988770	6070.619796	25.975130
194.229626	6080.563078	25.980148
194.208066	6089.551380	25.985165
194.432590	6108.298751	25.990183
194.999449	6114.831407	25.995200
194.606101	6137.739362	26.000218
194.837792	6143.176009	26.005236
195.111757	6154.461784	26.010253
195.265155	6165.703848	26.015271
195.601064	6184.922137	26.020288
195.694655	6193.579800	26.025306
196.116670	6196.386656	26.030324
196.533569	6227.794802	26.035341
196.510720	6232.604099	26.040359
196.711751	6218.278971	26.045376
197.120690	6240.901824	26.050394
197.280590	6257.011432	26.055412
197.539525	6253.062368	26.060429
197.542663	6260.193214	26.065447
198.149040	6260.830684	26.070464
198.005783	6281.290694	26.075482
198.427105	6282.707458	26.080500
198.678673	6293.601953	26.085517
198.702364	6317.420077	26.090535
198.845044	6319.154278	26.095552
198.931074	6307.384733	26.100570
199.202956	6327.972955	26.105588
199.428236	6335.778089	26.110605
199.605990	6355.499385	26.115623
200.053964	6341.069468	26.120640
200.301261	6347.402982	26.125658
200.510949	6365.344243	26.130676
200.571018	6361.026389	26.135693
200.574947	6360.827585	26.140711
200.896519	6374.810864	26.145728
200.550538	6378.659933	26.150746
200.932617	6389.265402	26.155764
201.314851	6400.864550	26.160781
201.263555	6410.755498	26.165799
201.602034	6407.710306	26.170816
201.922573	6433.073724	26.175834
201.658519	6453.820733	26.180852
201.965511	6453.107840	26.185869
202.093453	6474.724716	26.190887
202.451070	6468.439653	26.195904
202.914268	6484.918935	26.200922
203.133731	6492.961901	26.205940
203.632610	6498.306516	26.210957
203.646355	6506.537281	26.215975
203.763107	6497.280385	26.220992
203.844035	6521.454779	26.226010
203.962336	6530.700359	26.231028
204.154928	6535.309396	26.236045
204.518478	6549.477336	26.241063
205.054529	6558.605193	26.246080
204.744189	6562.397486	26.251098
205.085411	6571.153578	26.256116
205.504512	6579.648636	26.261133
205.562723	6581.827492	26.266151
205.710394	6588.275342	26.271168
205.919596	6616.778000	26.276186
205.982777	6610.202287	26.281204
206.458045	6613.317811	26.286221
206.556130	6643.386631	26.291239
206.670004	6649.533835	26.296256
206.822985	6663.881010	26.301274
206.886570	6673.863182	26.306292
207.447319	6670.112158	26.311309
207.295067	6695.603329	26.316327
207.656440	6697.139058	26.321344
207.891588	6712.090811	26.326362
208.100350	6721.644673	26.331380
208.448670	6738.056006	26.336397
208.235568	6753.944735	26.341415
208.934118	6752.366877	26.346432
208.962862	6761.175259	26.351450
209.291880	6761.455709	26.356468
210.228745	6776.556874	26.361485
210.271184	6778.105691	26.366503
210.540151	6772.486887	26.371520
211.121611	6775.401408	26.376538
211.136312	6782.185259	26.381556
211.205417	6776.448038	26.386573
211.001564	6774.637953	26.391591
211.048369	6775.705342	26.396608
211.339549	6764.641530	26.401626
210.984086	6780.362579	26.406644
211.662786	6786.804537	26.411661
211.715159	6792.927774	26.416679
211.418564	6811.439676	26.421696
211.919585	6822.172840	26.426714
212.135948	6839.842955	26.431732
212.340834	6839.334368	26.436749
212.536815	6865.811249	26.441767
212.947826	6873.110259	26.446784
213.304605	6881.631164	26.451802
213.572038	6893.062531	26.456820
213.589725	6891.642772	26.461837
213.609169	6894.919934	26.466855
213.956559	6907.857092	26.471872
214.009581	6919.131468	26.476890
214.481723	6931.935460	26.481908
214.814397	6938.963742	26.486925
214.494031	6946.874284	26.491943
215.128892	6968.253707	26.496960
215.005246	6978.599538	26.501978
214.868068	6984.916727	26.506996
215.495181	6991.054639	26.512013
215.707552	7008.650845	26.517031
215.585284	7026.719002	26.522048
216.185819	7036.337288	26.527066
216.533515	7052.502012	26.532084
216.974865	7066.591955	26.537101
216.876351	7058.480791	26.542119
217.142738	7081.322788	26.547136
217.782074	7097.168832	26.552154
217.458516	7108.677271	26.557172
218.029185	7098.551385	26.562189
217.942629	7110.344636	26.567207
218.216829	7131.164143	26.572224
218.652416	7128.237085	26.577242
218.588225	7142.939580	26.582260
219.117619	7157.336594	26.587277
219.288636	7161.551926	26.592295
219.424041	7168.211278	26.597312
219.524967	7176.820350	26.602330
219.745543	7190.581312	26.607348
220.511564	7194.805659	26.612365
220.382738	7208.086515	26.617383
220.744515	7216.425850	26.622400
220.766595	7216.937785	26.627418
221.037400	7230.644354	26.632436
221.097493	7239.795796	26.637453
221.082521	7247.383998	26.642471
221.864807	7257.641466	26.647488
221.980351	7252.692134	26.652506
221.853377	7269.297851	26.657524
222.155463	7273.637096	26.662541
222.532439	7293.299557	26.667559
222.556391	7288.522179	26.672576
222.995763	7308.094457	26.677594
222.996339	7316.657450	26.682612
223.338776	7322.418360	26.687629
223.780277	7338.770658	26.692647
223.535055	7344.412817	26.697664
224.094565	7345.103455	26.702682
224.182756	7361.974754	26.707700
224.476621	7361.606185	26.712717
224.834056	7371.636402	26.717735
224.835436	7383.885586	26.722752
225.220341	7396.453678	26.727770
225.210409	7407.444187	26.732788
225.412002	7408.276864	26.737805
225.344041	7432.367107	26.742823
225.715764	7437.924327	26.747840
226.142835	7444.260343	26.752858
226.237716	7464.490457	26.757876
226.537652	7464.743301	26.762893
226.559871	7485.899325	26.767911
226.991874	7499.485239	26.772928
227.516986	7498.344114	26.777946
227.246867	7514.712482	26.782964
227.604862	7522.678847	26.787981
227.665491	7522.436368	26.792999
227.919384	7554.431183	26.798016
228.408905	7561.836046	26.803034
228.407158	7572.690824	26.808052
228.861616	7589.063364	26.813069
228.801888	7598.223113	26.818087
228.981734	7618.522510	26.823104
229.291412	7632.237417	26.828122
229.220487	7647.322313	26.833140
229.805112	7661.516666	26.838157
229.926239	7688.597471	26.843175
230.034036	7688.038241	26.848192
230.585226	7698.923778	26.853210
230.776836	7721.028032	26.858228
230.874563	7717.326176	26.863245
231.181060	7743.228344	26.868263
231.312562	7754.593133	26.873280
231.883637	7768.478945	26.878298
231.857754	7781.555844	26.883316
232.245591	7788.487612	26.888333
232.529184	7797.577017	26.893351
232.747130	7819.037510	26.898368
233.244546	7832.909158	26.903386
233.189224	7835.389564	26.908404
233.499630	7841.883622	26.913421
233.795669	7861.560527	26.918439
233.746597	7863.158667	26.923456
233.825045	7875.178011	26.928474
234.298398	7897.299775	26.933492
234.455680	7900.275853	26.938509
234.885370	7919.862286	26.943527
234.818540	7934.871282	26.948544
235.531236	7934.158961	26.953562
235.650932	7951.151804	26.958580
235.638976	7960.301798	26.963597
236.147139	7978.760823	26.968615
236.325724	7981.358190	26.973632
236.718941	7985.066222	26.978650
236.851506	8014.456407	26.983668
237.118152	8019.797688	26.988685
237.325940	8018.633148	26.993703
237.451725	8034.990119	26.998720
237.897930	8047.969964	27.003738
237.820054	8047.818013	27.008756
238.110618	8051.271746	27.013773
238.320036	8061.134032	27.018791
238.406850	8077.654635	27.023808
238.815758	8082.133677	27.028826
238.865712	8091.939570	27.033844
239.052691	8105.133112	27.038861
239.158225	8106.785318	27.043879
239.406586	8133.704622	27.048896
240.063956	8135.892062	27.053914
240.120342	8140.860881	27.058932
240.230176	8155.627909	27.063949
240.440669	8171.227150	27.068967
240.770305	8194.001761	27.073984
241.199068	8202.758247	27.079002
241.003915	8212.228741	27.084020
241.396215	8219.801301	27.089037
241.754629	8229.647030	27.094055
242.142678	8242.436451	27.099072
242.445551	8248.110395	27.104090
242.843571	8270.331280	27.109108
242.994303	8288.156006	27.114125
243.185105	8282.071468	27.119143
243.602499	8294.570621	27.124160
243.914617	8291.149198	27.129178
243.694882	8309.642833	27.134196
243.921060	8323.567622	27.139213
244.577695	8337.944719	27.144231
244.296985	8345.772560	27.149248
244.731951	8369.684213	27.154266
245.056732	8375.296484	27.159284
245.009335	8387.844627	27.164301
245.245640	8407.286269	27.169319
245.461770	8419.263646	27.174336
245.982644	8430.792718	27.179354
245.819269	8446.083584	27.184372
246.378317	8466.023886	27.189389
246.757590	8474.956816	27.194407
246.815254	8498.850132	27.199424
247.437927	8507.046313	27.204442
247.628674	8521.910970	27.209460
247.778956	8530.612107	27.214477
248.034600	8523.213264	27.219495
248.167380	8547.390553	27.224512
248.662048	8555.703168	27.229530
248.671694	8561.565221	27.234548
248.891922	8578.384982	27.239565
249.330841	8585.290098	27.244583
249.564324	8600.431301	27.249600
249.434492	8620.101947	27.254618
249.938336	8630.468110	27.259636
250.497333	8640.698011	27.264653
250.705540	8653.652194	27.269671
250.728749	8658.596179	27.274688
250.859830	8657.134177	27.279706
251.060033	8671.176351	27.284724
251.126944	8681.062946	27.289741
251.695120	8684.753104	27.294759
251.696467	8720.367121	27.299776
252.064936	8713.795327	27.304794
251.977563	8707.163607	27.309812
252.415966	8733.269951	27.314829
252.910190	8759.455182	27.319847
252.845977	8771.714387	27.324864
253.016988	8774.781701	27.329882
252.880620	8798.215400	27.334900
253.038247	8816.654622	27.339917
253.812329	8829.825647	27.344935
254.139847	8861.998816	27.349952
254.441771	8858.110683	27.354970
254.844853	8871.494331	27.359988
255.517334	8882.804830	27.365005
255.601410	8893.679544	27.370023
255.742711	8913.549330	27.375040
256.127478	8919.106999	27.380058
256.772454	8923.026951	27.385076
256.458225	8931.296778	27.390093
256.977713	8940.085274	27.395111
256.809471	8950.462397	27.400128
256.768123	8967.336490	27.405146
257.022361	8989.086401	27.410164
257.400851	9010.296782	27.415181
257.775292	9025.375028	27.420199
258.039376	9045.706615	27.425216
258.048948	9054.136969	27.430234
258.503590	9067.939869	27.435252
258.837115	9089.803589	27.440269
259.462456	9101.408208	27.445287
259.438358	9108.095428	27.450304
259.729298	9117.188012	27.455322
260.485848	9133.672275	27.460340
260.438533	9144.862030	27.465357
260.702990	9141.326042	27.470375
260.769989	9158.448271	27.475392
261.118876	9174.223232	27.480410
261.148119	9173.707554	27.485428
261.027043	9192.365575	27.490445
261.486523	9213.578680	27.495463
261.857224	9225.752406	27.500480
261.733211	9242.723792	27.505498
262.227842	9259.760266	27.510516
262.401056	9280.367523	27.515533
263.114985	9286.607459	27.520551
263.336644	9313.568166	27.525568
263.617854	9321.466688	27.530586
264.159966	9335.285404	27.535604
264.009219	9362.084432	27.540621
264.668812	9361.095659	27.545639
264.738927	9378.408080	27.550656
264.802446	9390.990927	27.555674
265.139933	9394.608261	27.560692
265.361666	9405.511768	27.565709
265.852341	9422.429446	27.570727
265.925166	9428.276653	27.575744
265.934828	9437.797505	27.580762
266.523274	9442.779528	27.585780
266.479914	9473.741445	27.590797
266.976725	9477.687920	27.595815
266.912770	9493.228021	27.600832
267.195170	9510.377305	27.605850
267.753633	9522.759393	27.610868
267.580032	9548.597216	27.615885
268.195604	9555.436068	27.620903
268.185783	9565.028965	27.625920
268.346994	9582.976328	27.630938
268.852978	9604.938042	27.635956
268.841866	9639.800763	27.640973
269.634927	9636.632896	27.645991
269.749626	9661.248474	27.651008
270.288869	9673.318580	27.656026
270.501916	9687.581189	27.661044
271.088133	9695.972320	27.666061
271.041419	9696.429990	27.671079
270.990439	9719.303012	27.676096
271.435529	9729.244126	27.681114
272.290038	9739.751515	27.686132
271.805316	9762.101952	27.691149
272.445619	9773.220345	27.696167
272.648327	9789.655508	27.701184
272.660580	9797.708508	27.706202
273.227730	9817.823642	27.711220
273.193038	9836.877122	27.716237
273.193984	9843.655507	27.721255
273.518958	9860.129493	27.726272
273.972737	9887.597234	27.731290
274.247309	9895.772161	27.736308
274.431504	9926.763664	27.741325
275.038353	9941.961218	27.746343
275.689778	9950.978358	27.751360
275.595701	9982.700956	27.756378
276.255934	9988.194661	27.761396
276.497612	9992.223651	27.766413
276.896771	10007.977314	27.771431
276.473829	10011.549173	27.776448
276.959010	10033.176044	27.781466
277.847945	10035.754591	27.786484
277.483953	10046.947095	27.791501
278.065113	10054.457833	27.796519
278.487029	10066.417110	27.801536
278.567570	10086.353224	27.806554
278.729444	10097.181391	27.811572
278.543238	10115.099775	27.816589
279.042823	10122.276496	27.821607
279.532869	10136.547714	27.826624
279.464817	10149.697147	27.831642
279.937132	10163.836645	27.836660
279.893068	10173.772999	27.841677
280.257155	10191.141807	27.846695
280.644733	10196.236376	27.851712
281.021527	10223.807113	27.856730
281.231813	10230.008504	27.861748
281.276891	10248.458772	27.866765
281.537172	10256.222225	27.871783
281.690042	10283.151962	27.876800
281.775835	10312.314479	27.881818
282.245344	10317.222108	27.886836
282.731231	10345.175072	27.891853
282.566275	10364.021758	27.896871
283.431317	10380.773821	27.901888
283.723009	10407.218906	27.906906
284.186310	10420.315361	27.911924
284.019787	10441.533190	27.916941
284.370901	10450.352175	27.921959
284.789671	10469.563585	27.926976
285.168600	10490.236908	27.931994
285.909200	10505.348398	27.937012
285.785235	10512.396076	27.942029
286.111137	10528.741977	27.947047
286.513206	10541.360362	27.952064
286.413201	10567.328679	27.957082
286.846224	10576.000500	27.962100
287.378761	10599.570421	27.967117
287.862246	10606.648421	27.972135
288.223442	10618.615064	27.977152
288.363224	10645.754910	27.982170
288.500334	10641.352321	27.987188
288.659760	10675.544134	27.992205
288.821111	10683.503800	27.997223
289.365803	10689.896051	28.002240
289.575780	10708.859302	28.007258
290.215659	10721.984540	28.012276
290.156677	10741.019426	28.017293
290.399716	10745.480468	28.022311
290.487269	10771.988246	28.027328
290.651125	10798.245445	28.032346
291.364651	10800.426716	28.037364
291.302642	10820.366061	28.042381
291.451055	10844.250220	28.047399
292.046973	10863.861639	28.052416
292.061763	10881.572999	28.057434
292.280390	10903.393144	28.062452
292.694613	10928.307373	28.067469
293.366491	10945.744475	28.072487
293.555685	10974.117566	28.077504
293.675002	10990.546479	28.082522
294.053922	10996.548166	28.087540
294.583874	11016.716883	28.092557
294.789658	11035.911022	28.097575
295.439974	11040.625588	28.102592
295.528431	11063.314725	28.107610
295.811421	11071.078523	28.112628
296.037001	11077.464352	28.117645
296.242423	11097.210722	28.122663
296.712283	11091.847531	28.127680
296.684275	11116.722769	28.132698
297.127454	11127.242403	28.137716
297.271848	11148.636363	28.142733
297.576382	11161.812684	28.147751
298.243573	11167.980991	28.152768
298.521608	11197.990934	28.157786
298.476986	11201.400453	28.162804
298.874266	11211.515059	28.167821
299.156218	11227.001421	28.172839
299.687181	11233.397670	28.177856
299.417415	11247.782395	28.182874
300.036679	11260.306562	28.187892
300.531162	11281.478455	28.192909
300.389705	11286.781284	28.197927
300.833970	11325.129953	28.202944
301.252939	11329.395492	28.207962
301.446566	11359.662403	28.212980
301.582373	11375.665682	28.217997
301.344935	11393.838514	28.223015
301.982129	11418.485841	28.228032
301.868363	11449.335143	28.233050
302.349810	11463.267029	28.238068
302.923318	11496.047290	28.243085
303.092332	11525.562502	28.248103
303.872992	11546.413690	28.253120
304.060692	11566.029308	28.258138
304.440058	11587.356925	28.263156
304.841475	11596.142597	28.268173
305.216702	11622.518654	28.273191
305.689392	11633.782425	28.278208
305.583296	11657.915430	28.283226
305.729107	11668.587911	28.288244
306.481973	11676.342458	28.293261
306.433954	11721.717510	28.298279
306.895804	11724.865008	28.303296
306.898185	11746.653546	28.308314
307.370406	11757.411014	28.313332
307.753285	11777.115036	28.318349
307.956775	11804.728884	28.323367
308.803319	11816.630147	28.328384
308.975143	11844.354384	28.333402
308.958366	11854.666266	28.338420
309.642282	11865.043764	28.343437
309.963737	11880.857626	28.348455
310.609059	11896.939828	28.353472
310.346482	11905.307718	28.358490
310.588207	11914.273489	28.363508
310.738462	11948.906664	28.368525
310.896146	11983.331538	28.373543
311.449922	11966.284821	28.378560
311.323915	12000.940107	28.383578
311.982194	12018.266697	28.388596
312.342243	12033.305010	28.393613
312.376005	12060.328132	28.398631
313.100996	12072.326302	28.403648
313.082933	12091.951391	28.408666
313.554278	12112.661997	28.413684
313.816835	12120.761150	28.418701
314.000909	12142.212175	28.423719
314.805817	12173.071193	28.428736
315.018376	12180.824162	28.433754
314.986095	12188.848346	28.438772
315.370395	12223.620169	28.443789
315.831332	12239.246889	28.448807
315.956238	12243.560150	28.453824
316.082757	12273.661114	28.458842
316.556639	12289.319274	28.463860
316.919469	12319.802576	28.468877
317.166774	12342.427977	28.473895
317.750250	12358.981566	28.478912
317.813831	12386.246480	28.483930
317.945385	12402.584462	28.488948
318.587286	12414.090641	28.493965
319.079838	12427.252468	28.498983
319.210228	12456.403553	28.504000
319.570547	12483.339570	28.509018
320.101431	12497.349542	28.514036
320.535451	12512.051080	28.519053
320.683613	12533.918656	28.524071
321.237493	12549.920301	28.529088
321.168793	12562.793102	28.534106
321.484851	12581.919683	28.539124
322.416767	12586.133940	28.544141
322.305027	12612.662537	28.549159
322.986648	12633.992261	28.554176
322.971302	12645.816081	28.559194
323.124002	12660.812504	28.564212
323.511305	12686.162308	28.569229
323.979109	12707.389257	28.574247
324.267701	12716.583380	28.579264
324.431373	12730.916365	28.584282
324.497880	12763.574549	28.589300
325.170217	12786.712579	28.594317
325.283200	12791.918117	28.599335
325.629335	12821.957028	28.604352
326.097809	12840.953778	28.609370
326.359634	12861.248377	28.614388
326.700488	12883.337033	28.619405
326.806668	12897.624437	28.624423
327.333422	12917.937890	28.629440
327.399982	12933.332030	28.634458
327.637471	12961.042924	28.639476
328.554963	12993.318232	28.644493
328.759901	13002.833429	28.649511
328.896024	13024.543451	28.654528
329.754746	13029.253780	28.659546
330.710761	13025.280424	28.664564
331.346726	13026.236657	28.669581
331.625747	13032.771634	28.674599
332.170131	13021.493666	28.679616
332.390261	13012.908960	28.684634
332.479436	13027.189554	28.689652
332.369576	13036.126426	28.694669
332.535462	13027.478730	28.699687
333.002670	13025.106357	28.704704
332.824405	13035.790718	28.709722
332.963081	13057.322098	28.714740
333.190244	13063.866141	28.719757
333.344947	13091.805353	28.724775
333.395191	13104.917243	28.729792
333.596482	13137.157054	28.734810
334.059268	13156.223194	28.739828
334.493942	13190.877042	28.744845
334.577551	13214.820530	28.749863
335.027789	13236.943629	28.754880
335.376983	13267.300347	28.759898
335.660097	13290.972871	28.764916
336.224206	13307.535509	28.769933
336.241183	13339.134874	28.774951
336.574385	13370.402113	28.779968
337.073460	13390.974860	28.784986
336.981546	13423.049279	28.790004
337.660751	13451.843245	28.795021
338.241080	13479.447314	28.800039
338.693956	13506.188174	28.805056
339.213869	13533.260117	28.810074
339.617930	13556.621845	28.815092
340.146822	13571.322480	28.820109
340.323007	13599.876916	28.825127
340.678294	13616.115903	28.830144
340.934264	13620.774793	28.835162
341.206422	13662.294891	28.840180
341.380763	13681.368695	28.845197
341.764429	13700.038807	28.850215
341.762742	13732.908990	28.855232
342.493837	13749.418244	28.860250
342.694285	13787.871040	28.865268
343.562229	13802.076464	28.870285
343.611054	13824.711598	28.875303
343.973021	13841.893103	28.880320
344.532939	13851.357181	28.885338
344.551869	13886.139972	28.890356
345.082617	13911.566177	28.895373
345.471043	13932.862496	28.900391
345.732298	13952.857257	28.905408
346.125854	13968.841974	28.910426
346.574553	13988.449731	28.915444
348.062895	13985.997826	28.920461
349.489732	13967.485336	28.925479
349.591534	13944.236870	28.930496
350.083572	13937.487485	28.935514
350.459485	13929.883050	28.940532
350.504801	13902.588943	28.945549
350.272960	13892.506360	28.950567
350.348951	13902.225688	28.955584
350.266483	13889.282550	28.960602
350.556934	13900.663158	28.965620
351.116031	13892.994912	28.970637
351.108659	13909.924794	28.975655
351.055271	13924.134587	28.980672
351.218806	13937.500516	28.985690
351.508645	13965.773629	28.990708
351.857838	13998.659411	28.995725
352.151995	14009.340994	29.000743
352.231032	14035.320652	29.005760
352.657665	14052.786470	29.010778
352.930412	14086.088838	29.015796
353.077623	14098.407220	29.020813
353.417796	14138.827242	29.025831
353.503713	14172.802993	29.030848
353.809965	14198.315835	29.035866
354.293480	14232.745240	29.040884
354.558500	14267.938182	29.045901
355.103899	14298.241681	29.050919
355.321289	14328.247999	29.055936
355.726333	14361.251809	29.060954
355.992373	14396.129712	29.065972
356.668908	14414.391528	29.070989
357.036723	14441.186159	29.076007
357.810259	14475.792573	29.081024
358.426170	14499.970687	29.086042
358.523888	14522.211270	29.091060
359.025951	14546.983634	29.096077
359.292226	14571.695115	29.101095
359.923114	14590.382323	29.106112
360.137779	14604.883804	29.111130
360.312777	14637.738305	29.116148
360.786357	14652.878126	29.121165
361.329638	14672.926773	29.126183
361.447494	14712.547825	29.131200
362.089533	14727.862795	29.136218
362.132013	14751.529785	29.141236
362.401970	14770.672569	29.146253
362.818539	14797.300350	29.151271
363.153316	14820.153236	29.156288
363.741700	14832.047559	29.161306
364.182827	14876.731761	29.166324
364.512796	14877.404097	29.171341
365.251908	14893.015896	29.176359
364.922370	14917.944804	29.181376
365.714016	14933.782668	29.186394
365.929335	14969.412408	29.191412
366.092830	14990.237899	29.196429
366.605121	15003.244725	29.201447
367.139568	15028.119477	29.206464
367.482258	15047.595822	29.211482
367.506455	15073.181248	29.216500
367.577654	15082.810969	29.221517
368.270045	15094.334377	29.226535
368.166798	15133.731081	29.231552
368.575711	15149.883944	29.236570
369.118696	15179.029000	29.241588
370.247620	15199.640410	29.246605
370.699985	15213.826107	29.251623
371.228529	15219.426984	29.256640
371.985505	15226.453555	29.261658
372.021139	15237.167257	29.266676
372.236697	15246.664258	29.271693
372.723850	15254.815600	29.276711
372.690627	15275.301349	29.281728
373.150262	15287.080060	29.286746
373.185450	15299.698994	29.291764
373.623278	15327.329222	29.296781
373.985942	15342.356428	29.301799
374.181472	15360.098811	29.306816
374.369344	15383.304622	29.311834
374.560981	15405.718785	29.316852
374.808952	15447.162563	29.321869
375.192187	15469.097262	29.326887
375.364688	15503.313986	29.331904
376.253640	15536.377249	29.336922
376.221405	15575.013813	29.341940
376.729804	15605.032941	29.346957
376.903254	15635.360181	29.351975
377.350514	15680.648886	29.356992
378.337090	15703.364094	29.362010
378.449865	15733.519929	29.367028
379.087379	15754.593207	29.372045
379.646556	15787.520916	29.377063
379.776361	15811.523890	29.382080
380.102951	15823.517293	29.387098
380.609485	15867.438579	29.392116
380.872587	15883.519701	29.397133
381.447837	15898.247677	29.402151
381.687736	15926.153004	29.407168
382.599138	15949.833057	29.412186
382.771304	15978.433904	29.417204
382.912140	15991.869407	29.422221
383.248368	16021.203319	29.427239
384.101354	16033.929608	29.432256
384.423431	16061.373436	29.437274
384.605094	16087.870350	29.442292
384.714453	16101.104895	29.447309
385.148716	16126.830439	29.452327
385.074046	16163.441004	29.457344
385.927133	16183.402731	29.462362
386.253311	16214.465521	29.467380
386.707441	16237.117276	29.472397
387.385872	16253.982973	29.477415
387.544580	16299.301473	29.482432
387.768391	16300.019335	29.487450
388.057468	16316.068724	29.492468
388.371600	16351.883043	29.497485
388.795338	16376.380143	29.502503
389.283915	16395.979621	29.507520
390.022430	16423.771854	29.512538
390.180909	16437.509619	29.517556
390.073547	16468.381803	29.522573
390.986552	16481.127640	29.527591
390.766173	16503.919942	29.532608
391.315485	16537.135342	29.537626
391.781820	16578.168579	29.542644
392.097857	16590.231184	29.547661
392.837665	16623.457946	29.552679
393.103284	16652.960790	29.557696
393.577386	16668.726371	29.562714
393.973502	16711.765210	29.567732
394.378181	16722.179927	29.572749
395.078780	16749.737285	29.577767
394.992567	16785.409144	29.582784
395.498447	16803.393767	29.587802
395.911886	16834.935189	29.592820
396.464660	16861.712255	29.597837
396.789791	16882.122763	29.602855
396.931494	16917.606066	29.607872
397.914759	16936.974275	29.612890
398.362647	16966.690187	29.617908
398.508399	16981.304198	29.622925
399.064392	16994.623445	29.627943
399.222877	17031.706150	29.632960
400.074783	17047.460734	29.637978
400.540217	17077.627763	29.642996
400.976519	17092.977204	29.648013
401.545367	17094.205036	29.653031
401.423873	17132.967095	29.658048
401.545441	17147.379229	29.663066
401.982307	17175.391543	29.668084
402.314232	17199.041664	29.673101
402.771644	17218.036775	29.678119
403.241670	17247.404257	29.683136
403.437255	17279.874143	29.688154
404.367454	17298.649738	29.693172
404.525022	17333.449631	29.698189
404.847082	17351.175231	29.703207
405.151066	17377.865879	29.708224
405.724136	17398.520024	29.713242
406.175960	17426.001707	29.718260
406.326427	17465.422395	29.723277
406.842364	17471.924091	29.728295
407.288647	17510.263772	29.733312
407.768480	17533.396381	29.738330
407.938679	17556.435063	29.743348
408.735055	17579.027372	29.748365
409.060875	17599.670793	29.753383
409.135698	17628.414413	29.758400
409.602777	17638.943426	29.763418
410.170838	17668.446277	29.768436
410.093379	17700.670804	29.773453
410.805902	17710.295054	29.778471
411.217208	17746.375064	29.783488
411.717723	17767.674699	29.788506
412.126362	17791.830212	29.793524
412.506345	17818.868944	29.798541
412.805226	17834.893159	29.803559
412.869069	17866.765215	29.808576
413.464920	17893.494889	29.813594
414.031991	17909.783523	29.818612
414.094343	17948.828551	29.823629
414.668753	17982.256048	29.828647
415.423601	18012.552996	29.833664
415.601394	18044.986771	29.838682
416.035949	18061.836035	29.843700
416.150242	18088.520732	29.848717
416.906709	18116.379107	29.853735
417.127441	18158.693441	29.858752
417.510684	18183.272500	29.863770
418.345280	18213.155961	29.868788
418.437660	18236.192896	29.873805
419.308042	18265.916429	29.878823
419.457365	18302.184749	29.883840
419.954011	18322.027123	29.888858
420.635215	18354.619127	29.893876
420.876083	18375.033813	29.898893
421.592776	18411.602142	29.903911
421.722851	18434.040454	29.908928
422.011048	18451.544168	29.913946
422.836279	18480.919799	29.918964
422.752754	18511.269021	29.923981
423.505542	18536.161808	29.928999
423.675793	18556.700190	29.934016
423.847946	18587.871032	29.939034
424.706880	18625.168386	29.944052
424.649089	18655.838202	29.949069
425.074197	18675.990856	29.954087
425.603050	18708.495279	29.959104
426.081294	18745.199239	29.964122
427.100281	18783.270698	29.969140
427.198718	18811.883214	29.974157
427.791243	18825.327757	29.979175
428.151994	18859.465614	29.984192
428.472998	18885.027773	29.989210
429.168261	18909.903554	29.994228
429.517866	18938.819601	29.999245
429.988986	18965.454855	30.004263
430.267836	18991.007369	30.009280
430.618119	19013.987434	30.014298
431.450938	19030.724297	30.019316
431.285664	19058.383579	30.024333
431.957477	19079.498274	30.029351
432.421231	19111.165062	30.034368
432.772776	19146.984610	30.039386
433.130578	19159.812092	30.044404
432.974502	19184.590483	30.049421
434.040587	19204.215694	30.054439
434.726461	19233.535032	30.059456
435.024910	19267.496300	30.064474
435.429448	19285.696627	30.069492
435.522881	19303.473291	30.074509
436.015459	19329.575803	30.079527
436.320792	19362.940087	30.084544
436.464271	19387.211597	30.089562
437.266963	19429.993784	30.094580
437.452060	19462.470691	30.099597
437.935180	19479.569681	30.104615
438.441197	19523.412449	30.109632
438.537414	19561.548977	30.114650
439.061571	19588.969817	30.119668
439.613202	19627.598947	30.124685
440.030967	19667.555111	30.129703
440.664741	19699.685414	30.134720
441.149190	19719.705943	30.139738
441.985378	19751.102473	30.144756
442.486425	19773.012704	30.149773
442.994813	19805.919171	30.154791
443.414240	19829.860372	30.159808
443.477997	19848.377487	30.164826
444.218723	19873.303874	30.169844
444.565466	19906.622562	30.174861
444.932471	19939.962111	30.179879
445.659194	19968.915665	30.184896
446.033231	20001.435250	30.189914
446.725650	20024.624133	30.194932
446.840574	20047.944039	30.199949
447.653453	20069.250619	30.204967
447.794354	20098.677315	30.209984
448.396789	20124.284867	30.215002
448.824180	20141.102096	30.220020
448.983861	20178.939043	30.225037
449.209548	20204.009441	30.230055
449.952146	20244.581544	30.235072
449.813727	20269.611621	30.240090
450.633005	20309.514908	30.245108
450.542049	20343.729162	30.250125
451.224370	20367.510391	30.255143
452.119232	20408.411852	30.260160
452.381248	20443.574147	30.265178
452.949855	20479.919721	30.270196
453.315812	20514.884491	30.275213
453.389902	20547.245886	30.280231
454.218743	20584.983108	30.285248
454.577478	20612.465572	30.290266
455.335611	20646.753112	30.295284
455.495180	20686.002911	30.300301
456.292288	20710.399536	30.305319
456.984285	20726.941742	30.310336
457.054750	20770.942847	30.315354
457.598563	20777.302905	30.320372
457.999952	20807.758484	30.325389
458.339789	20846.685041	30.330407
458.508464	20870.916250	30.335424
459.152806	20894.551161	30.340442
459.540910	20910.735223	30.345460
459.692734	20949.439981	30.350477
460.008125	20978.717281	30.355495
460.595166	21019.137408	30.360512
460.774696	21056.418101	30.365530
461.193323	21095.179940	30.370548
461.646400	21135.818593	30.375565
462.486439	21175.106505	30.380583
463.064956	21208.798194	30.385600
463.466558	21256.162273	30.390618
464.107403	21281.449011	30.395636
464.596900	21316.077325	30.400653
465.284268	21355.678253	30.405671
466.040586	21370.695266	30.410688
466.059125	21411.044739	30.415706
466.965486	21438.373282	30.420724
467.481967	21454.257087	30.425741
467.703153	21498.489412	30.430759
468.050310	21526.367130	30.435776
468.786779	21565.339386	30.440794
469.241148	21577.026088	30.445812
469.360962	21607.719455	30.450829
469.712668	21643.460423	30.455847
470.565703	21666.826199	30.460864
470.864127	21709.563835	30.465882
471.162683	21742.271140	30.470900
471.787189	21775.166005	30.475917
472.199035	21805.826622	30.480935
472.704384	21830.006461	30.485952
473.345755	21877.917015	30.490970
473.893286	21895.954267	30.495988
474.214400	21923.991202	30.501005
474.705339	21966.328706	30.506023
475.399343	21988.586189	30.511040
475.904037	22017.463530	30.516058
476.179906	22061.213814	30.521076
476.754924	22083.097384	30.526093
476.894931	22123.765626	30.531111
477.546696	22146.128510	30.536128
477.881756	22186.232645	30.541146
478.328943	22216.225284	30.546164
478.965018	22256.228873	30.551181
479.067619	22287.207475	30.556199
479.845003	22320.823401	30.561216
480.163395	22357.922808	30.566234
480.983896	22380.299311	30.571252
481.291241	22424.309432	30.576269
481.522347	22458.469486	30.581287
482.202534	22473.450070	30.586304
482.635773	22513.537820	30.591322
483.190082	22538.574162	30.596340
483.467143	22574.398442	30.601357
483.760464	22602.794648	30.606375
484.563741	22627.949778	30.611392
484.882889	22674.984710	30.616410
485.238068	22694.471223	30.621428
485.620323	22730.702047	30.626445
486.195782	22775.336754	30.631463
486.956556	22802.229327	30.636480
487.160409	22834.678317	30.641498
487.923833	22874.771092	30.646516
488.228885	22897.700658	30.651533
488.616383	22939.524031	30.656551
489.250765	22973.567396	30.661568
489.717238	23010.047723	30.666586
490.124005	23052.182589	30.671604
490.694655	23096.759897	30.676621
491.099078	23127.701514	30.681639
491.880324	23166.640671	30.686656
492.383618	23192.825887	30.691674
493.281351	23218.764791	30.696692
493.747796	23230.727265	30.701709
493.914403	23280.292987	30.706727
494.854403	23303.668615	30.711744
495.188560	23339.068868	30.716762
495.587716	23364.490404	30.721780
496.583627	23387.986425	30.726797
497.083844	23423.779442	30.731815
497.337714	23451.767578	30.736832
497.643504	23469.926275	30.741850
498.136783	23511.322368	30.746868
498.732004	23532.249312	30.751885
498.847178	23570.021935	30.756903
499.518748	23605.574611	30.761920
499.644837	23637.873802	30.766938
500.187659	23675.512387	30.771956
500.629840	23711.983237	30.776973
501.019972	23749.875531	30.781991
501.725174	23782.430911	30.787008
502.265016	23815.994133	30.792026
502.564792	23858.034760	30.797044
503.547482	23896.728592	30.802061
503.884429	23942.690067	30.807079
504.330728	23968.026294	30.812096
504.981888	24005.045044	30.817114
505.343077	24045.015820	30.822132
506.010881	24075.263558	30.827149
506.596621	24105.696929	30.832167
507.204138	24147.393131	30.837184
507.188194	24177.315969	30.842202
507.929093	24213.616720	30.847220
508.620740	24249.557549	30.852237
508.748440	24280.661288	30.857255
509.706276	24311.599767	30.862272
509.880590	24347.067903	30.867290
510.216210	24368.023129	30.872308
510.735065	24401.477505	30.877325
511.179133	24438.835094	30.882343
511.662714	24461.815679	30.887360
512.368363	24510.995318	30.892378
512.671094	24537.534514	30.897396
512.987587	24567.809221	30.902413
513.337923	24611.967439	30.907431
514.039572	24654.928427	30.912448
514.808182	24683.727637	30.917466
514.854538	24729.902305	30.922484
515.960940	24758.336696	30.927501
516.447139	24799.505685	30.932519
516.723107	24829.727478	30.937536
517.148605	24874.356534	30.942554
517.697219	24909.484294	30.947572
518.475168	24940.149382	30.952589
518.881298	24988.313206	30.957607
519.439566	25022.349464	30.962624
519.945596	25065.460880	30.967642
520.330456	25102.828671	30.972660
521.160331	25143.364820	30.977677
521.053110	25187.412399	30.982695
522.011034	25224.508011	30.987712
522.551687	25266.813327	30.992730
523.113864	25308.476468	30.997748
523.785140	25345.904761	31.002765
524.296448	25378.585677	31.007783
524.808264	25414.189907	31.012800
525.269909	25452.043352	31.017818
525.775257	25494.993760	31.022836
526.419227	25533.242164	31.027853
527.162111	25567.939464	31.032871
527.660320	25592.208905	31.037888
528.007511	25642.426738	31.042906
528.215457	25681.078960	31.047924
529.058899	25710.974913	31.052941
529.675278	25766.462919	31.057959
530.036296	25795.741069	31.062976
530.563923	25829.555478	31.067994
531.404645	25885.729758	31.073012
531.829204	25910.955950	31.078029
532.159724	25949.564875	31.083047
532.785115	25988.963539	31.088064
533.548660	26023.151998	31.093082
533.700229	26059.939994	31.098100
534.972928	26099.791208	31.103117
535.162186	26131.119562	31.108135
535.577740	26176.157181	31.113152
536.465422	26190.741928	31.118170
536.499031	26237.806868	31.123188
537.226128	26268.232097	31.128205
537.443491	26302.479004	31.133223
538.175903	26340.845240	31.138240
538.771510	26363.935195	31.143258
538.804709	26404.245363	31.148276
539.926312	26425.950975	31.153293
539.797094	26471.339319	31.158311
540.147739	26512.689508	31.163328
541.039361	26543.485318	31.168346
541.388149	26590.114276	31.173364
542.006711	26625.174006	31.178381
542.213811	26671.296362	31.183399
543.057937	26715.054792	31.188416
543.496716	26758.146028	31.193434
543.958242	26798.747413	31.198452
544.533771	26841.233320	31.203469
544.724667	26887.319485	31.208487
545.623071	26943.551310	31.213504
546.032543	26989.252372	31.218522
546.555142	27027.102192	31.223540
546.845103	27084.186947	31.228557
547.486661	27139.783624	31.233575
548.308048	27176.239801	31.238592
549.060594	27223.548422	31.243610
549.386243	27264.691022	31.248628
550.267339	27311.536662	31.253645
550.768607	27353.448809	31.258663
551.250160	27409.249167	31.263680
552.092011	27441.791041	31.268698
552.610905	27484.064706	31.273716
553.384295	27523.196968	31.278733
553.818453	27569.658383	31.283751
554.578169	27597.547208	31.288768
555.386105	27644.615829	31.293786
555.759744	27683.170837	31.298804
556.527981	27712.924153	31.303821
557.136729	27755.590754	31.308839
557.509147	27777.556987	31.313856
558.120656	27812.357284	31.318874
558.560809	27850.991916	31.323892
559.028517	27888.462511	31.328909
559.305749	27935.365968	31.333927
559.741744	27970.467164	31.338944
560.363959	28013.661753	31.343962
561.009327	28059.903424	31.348980
561.650181	28100.693831	31.353997
562.116820	28141.031482	31.359015
562.311828	28192.001634	31.364032
563.112097	28239.695640	31.369050
563.369219	28281.417447	31.374068
564.257955	28321.757654	31.379085
565.112104	28366.545599	31.384103
565.551508	28412.502777	31.389120
566.254433	28444.143032	31.394138
566.340450	28500.377317	31.399156
567.421816	28537.912409	31.404173
567.763549	28573.209569	31.409191
568.422022	28631.634894	31.414208
569.082772	28653.406694	31.419226
569.421609	28699.248335	31.424244
569.888407	28733.241636	31.429261
570.327060	28770.523501	31.434279
570.785377	28812.452579	31.439296
571.539257	28845.650300	31.444314
572.110392	28892.531780	31.449332
572.815739	28927.938837	31.454349
573.425245	28965.888885	31.459367
573.827856	29002.450562	31.464384
574.231757	29041.981012	31.469402
574.704943	29097.071516	31.474420
575.421819	29132.253414	31.479437
575.885545	29186.924975	31.484455
576.165600	29230.842322	31.489472
577.084879	29281.623326	31.494490
577.532056	29328.169660	31.499508
578.246556	29375.585987	31.504525
578.679170	29426.983906	31.509543
579.291613	29476.519011	31.514560
580.349994	29508.459311	31.519578
580.685755	29559.011061	31.524596
581.723739	29600.963319	31.529613
582.194625	29649.744579	31.534631
582.488287	29689.057775	31.539648
583.738341	29722.148327	31.544666
584.096284	29772.318987	31.549684
584.531914	29814.258993	31.554701
585.333293	29859.259614	31.559719
585.573623	29898.206739	31.564736
586.250760	29924.807869	31.569754
586.871832	29971.167603	31.574772
587.358986	30021.162433	31.579789
588.154162	30063.288513	31.584807
588.444062	30102.174648	31.589824
589.296695	30142.132731	31.594842
589.514086	30188.785890	31.599860
590.119591	30239.074579	31.604877
591.175497	30279.823279	31.609895
591.196020	30334.455811	31.614912
592.015778	30376.277775	31.619930
592.516189	30424.670539	31.624948
593.239025	30471.888585	31.629965
593.840197	30525.081811	31.634983
594.372479	30571.942801	31.640000
595.131623	30609.682160	31.645018
595.599202	30656.172304	31.650036
596.009011	30706.544032	31.655053
596.813075	30758.660813	31.660071
596.786598	30800.856617	31.665088
597.848262	30844.037607	31.670106
598.499552	30903.751966	31.675124
598.993572	30945.876281	31.680141
599.653113	30990.637843	31.685159
599.709900	31035.848555	31.690176
600.806000	31076.101123	31.695194
600.959955	31137.707990	31.700212
601.364637	31183.574502	31.705229
602.335842	31228.548706	31.710247
602.873572	31277.053101	31.715264
603.443282	31323.856698	31.720282
604.252869	31370.139949	31.725300
604.687909	31414.315876	31.730317
605.370766	31468.085460	31.735335
605.672667	31513.458614	31.740352
606.777193	31560.708856	31.745370
606.934790	31618.041014	31.750388
607.696789	31671.258060	31.755405
608.495519	31716.809558	31.760423
609.052780	31760.369608	31.765440
609.777044	31804.342914	31.770458
609.912071	31865.121760	31.775476
611.064569	31914.794185	31.780493
611.222669	31962.762139	31.785511
611.903464	32019.712911	31.790528
612.500525	32064.511000	31.795546
613.348204	32119.608798	31.800564
613.904590	32178.061506	31.805581
614.658194	32221.917776	31.810599
615.018583	32275.906857	31.815616
615.637564	32325.657610	31.820634
616.323529	32388.346071	31.825652
617.003476	32441.703199	31.830669
617.735538	32486.236631	31.835687
618.090267	32547.586683	31.840704
619.203228	32590.836621	31.845722
619.752038	32637.432929	31.850740
620.306932	32701.883574	31.855757
620.892774	32740.364733	31.860775
621.451663	32798.770384	31.865792
622.066623	32843.589812	31.870810
622.732215	32907.672137	31.875828
623.342360	32956.105331	31.880845
624.274929	33000.817863	31.885863
624.408583	33061.246683	31.890880
625.407673	33108.540242	31.895898
626.339996	33151.188350	31.900916
626.603188	33215.919164	31.905933
627.110633	33256.333883	31.910951
627.587200	33306.622558	31.915968
628.361803	33370.468644	31.920986
628.622065	33428.570995	31.926004
629.569348	33468.276225	31.931021
630.219725	33524.712144	31.936039
630.627899	33596.200927	31.941056
631.369273	33632.901844	31.946074
632.427624	33690.163962	31.951092
632.924332	33755.498097	31.956109
633.451952	33792.455666	31.961127
634.158231	33831.903805	31.966144
634.688052	33880.302058	31.971162
635.197834	33930.762311	31.976180
635.422599	33973.761668	31.981197
636.564130	34029.334511	31.986215
636.744637	34077.866207	31.991232
637.309596	34124.727385	31.996250
638.284728	34190.020149	32.001268
638.597746	34238.367272	32.006285
639.239197	34280.098317	32.011303
639.918301	34342.311345	32.016320
640.522138	34394.279214	32.021338
641.320624	34449.137253	32.026356
641.991537	34504.089879	32.031373
642.656783	34552.865775	32.036391
642.918618	34620.941048	32.041408
643.466659	34676.249578	32.046426
644.372627	34736.884676	32.051444
644.928072	34808.058863	32.056461
645.770685	34841.637680	32.061479
646.336498	34915.572533	32.066496
647.181728	34978.428309	32.071514
647.478570	35025.476601	32.076532
648.191665	35105.177456	32.081549
648.993895	35148.286524	32.086567
649.527163	35213.713579	32.091584
650.372820	35273.494773	32.096602
651.297328	35330.730272	32.101620
651.971877	35383.947980	32.106637
652.739136	35440.698126	32.111655
653.531950	35505.501708	32.116672
654.060363	35547.548734	32.121690
654.818104	35594.123238	32.126708
655.376768	35658.034578	32.131725
656.226701	35701.550521	32.136743
656.785078	35753.599239	32.141760
657.065606	35804.480039	32.146778
658.352338	35864.357073	32.151796
658.448857	35919.580825	32.156813
659.038225	35981.305054	32.161831
659.489767	36029.086689	32.166848
660.326320	36091.689496	32.171866
660.885070	36153.047176	32.176884
661.307512	36216.622894	32.181901
662.218190	36272.782328	32.186919
662.734686	36337.864888	32.191936
663.485694	36392.262348	32.196954
664.226034	36452.983664	32.201972
664.927554	36513.448096	32.206989
665.437921	36576.757353	32.212007
666.336512	36648.816494	32.217024
666.813824	36703.137148	32.222042
667.758095	36757.695787	32.227060
668.039623	36831.720643	32.232077
669.010087	36887.227793	32.237095
669.425640	36934.205793	32.242112
670.081221	36995.391901	32.247130
670.731483	37042.485761	32.252148
671.509455	37091.799787	32.257165
672.513737	37145.344254	32.262183
672.648425	37210.459460	32.267200
673.214324	37263.534900	32.272218
673.822100	37317.174583	32.277236
674.346444	37382.751854	32.282253
675.156481	37441.371870	32.287271
675.916512	37501.907801	32.292288
676.492745	37567.661999	32.297306
677.314153	37621.383732	32.302324
677.852528	37692.807822	32.307341
678.482907	37751.626229	32.312359
679.378465	37813.655312	32.317376
679.968200	37881.135049	32.322394
680.857772	37949.789253	32.327412
681.089615	38015.437633	32.332429
682.204487	38071.420788	32.337447
682.851528	38143.188972	32.342464
683.351252	38203.046736	32.347482
684.697684	38260.286558	32.352500
685.260861	38322.496574	32.357517
686.038710	38375.830313	32.362535
686.590983	38436.104678	32.367552
687.611229	38493.963281	32.372570
688.278244	38551.515671	32.377588
688.678460	38616.910949	32.382605
689.499814	38667.145086	32.387623
689.888273	38728.198689	32.392640
690.378886	38796.981356	32.397658
691.503731	38852.752653	32.402676
691.899255	38911.730754	32.407693
692.612326	38975.868212	32.412711
693.232981	39042.149301	32.417728
694.113080	39105.606286	32.422746
695.191903	39173.297134	32.427764
695.628558	39245.073530	32.432781
696.165760	39296.240947	32.437799
696.891402	39363.529933	32.442816
697.513152	39436.805614	32.447834
698.225316	39497.441468	32.452852
698.892245	39558.907854	32.457869
699.742117	39617.746687	32.462887
700.624471	39681.550799	32.467904
701.013244	39750.804527	32.472922
701.746823	39817.193659	32.477940
702.392770	39883.393586	32.482957
702.996185	39952.481502	32.487975
704.071223	40010.019609	32.492992
704.498002	40077.111434	32.498010
705.142028	40143.782593	32.503028
705.676002	40206.062513	32.508045
706.416406	40260.921975	32.513063
707.208780	40324.465290	32.518080
707.856598	40395.263616	32.523098
708.716616	40438.823317	32.528116
709.558084	40505.574842	32.533133
709.765078	40575.721867	32.538151
710.872753	40629.458033	32.543168
711.211858	40693.984787	32.548186
712.110519	40747.984839	32.553204
712.535504	40817.839531	32.558221
713.315343	40886.890529	32.563239
713.946726	40946.932545	32.568256
714.676866	41021.114004	32.573274
715.685752	41085.455174	32.578292
716.149208	41157.377286	32.583309
716.606447	41221.481935	32.588327
717.751948	41288.186539	32.593344
718.325073	41357.726527	32.598362
719.079916	41420.377848	32.603380
719.824214	41491.625844	32.608397
720.396408	41569.979243	32.613415
721.321725	41635.411322	32.618432
722.007798	41698.850512	32.623450
723.243486	41760.745242	32.628468
723.556112	41843.282540	32.633485
724.234650	41904.613593	32.638503
725.140955	41966.876920	32.643520
725.599110	42037.037252	32.648538
726.727297	42100.546323	32.653556
727.349295	42173.683884	32.658573
727.764699	42251.983350	32.663591
728.681598	42322.866668	32.668608
729.418258	42388.536678	32.673626
730.624100	42452.662377	32.678644
731.185823	42519.868458	32.683661
731.753731	42592.486501	32.688679
732.622332	42652.850000	32.693696
732.987418	42717.520592	32.698714
734.010643	42798.542538	32.703732
734.509390	42863.902113	32.708749
735.268586	42937.352278	32.713767
736.077434	43008.239851	32.718784
736.862721	43084.045920	32.723802
738.043942	43146.178278	32.728820
738.444488	43222.418419	32.733837
739.072663	43294.909960	32.738855
739.707436	43351.253453	32.743872
740.162126	43430.444705	32.748890
741.156977	43504.055339	32.753908
742.125990	43582.342105	32.758925
743.051429	43641.681139	32.763943
743.894704	43717.140077	32.768960
744.209842	43792.267033	32.773978
745.155304	43854.546727	32.778996
745.778676	43925.748341	32.784013
746.486689	44001.728462	32.789031
747.579066	44049.582017	32.794048
747.883077	44112.024691	32.799066
748.596571	44187.108868	32.804084
749.376714	44241.274416	32.809101
749.725210	44306.527717	32.814119
750.637693	44372.035327	32.819136
751.229789	44452.486976	32.824154
752.443295	44513.947188	32.829172
753.396076	44583.707888	32.834189
754.083351	44649.299717	32.839207
754.751838	44701.484449	32.844224
755.289347	44763.674624	32.849242
756.161800	44833.237753	32.854260
756.862705	44899.140666	32.859277
757.413177	44979.888457	32.864295
758.369584	45033.129334	32.869312
759.141236	45112.571191	32.874330
759.780820	45183.955202	32.879348
760.325297	45265.184787	32.884365
760.987975	45345.932186	32.889383
762.041519	45419.560538	32.894400
762.411222	45495.853428	32.899418
763.379417	45570.710594	32.904436
764.128094	45652.985260	32.909453
764.765356	45734.088684	32.914471
765.823251	45796.247027	32.919488
766.307096	45889.316620	32.924506
767.561123	45959.820437	32.929524
768.435615	46033.820611	32.934541
768.980056	46111.470206	32.939559
769.865100	46183.046381	32.944576
770.547658	46257.160080	32.949594
771.271362	46337.921280	32.954612
772.198917	46423.953855	32.959629
772.648827	46490.874456	32.964647
773.746693	46562.790591	32.969664
774.329619	46653.617913	32.974682
775.318974	46718.734048	32.979700
776.103433	46802.342985	32.984717
776.654003	46871.993875	32.989735
777.510618	46946.076471	32.994752
778.258085	47032.784328	32.999770
778.936690	47110.495867	33.004788
779.979050	47184.057710	33.009805
780.487547	47282.986597	33.014823
781.434198	47341.426198	33.019840
782.119233	47437.759598	33.024858
782.959331	47515.983593	33.029876
783.784908	47586.650508	33.034893
784.476767	47664.040557	33.039911
785.820885	47749.861873	33.044928
786.508198	47820.605375	33.049946
787.296941	47902.764320	33.054964
787.714472	47981.871691	33.059981
788.479705	48044.223426	33.064999
789.571076	48116.339427	33.070016
790.134431	48182.730946	33.075034
791.224868	48253.822200	33.080052
791.816685	48311.598949	33.085069
792.592486	48390.010598	33.090087
793.258097	48462.893107	33.095104
794.353246	48530.583309	33.100122
794.904467	48596.912054	33.105140
795.713047	48662.651053	33.110157
796.388982	48744.560513	33.115175
797.212360	48805.144992	33.120192
797.759779	48887.110276	33.125210
798.481683	48964.690565	33.130228
799.363464	49031.681442	33.135245
799.777898	49126.637726	33.140263
800.547215	49207.559436	33.145280
801.575820	49283.760708	33.150298
802.334224	49366.448776	33.155316
803.218544	49449.350693	33.160333
804.190903	49539.338850	33.165351
805.225948	49615.685676	33.170368
805.720990	49695.744481	33.175386
806.534889	49783.108455	33.180404
807.423313	49852.445940	33.185421
808.083892	49949.096680	33.190439
809.333160	50021.296290	33.195456
810.069460	50098.118744	33.200474
810.439450	50171.752714	33.205492
810.951553	50261.729427	33.210509
811.433997	50367.072978	33.215527
812.801965	50448.015493	33.220544
813.688365	50542.670689	33.225562
814.370734	50643.329430	33.230580
815.487319	50720.725174	33.235597
816.452946	50811.206809	33.240615
817.389410	50896.593873	33.245632
818.016580	50976.173501	33.250650
818.933839	51067.263723	33.255668
819.918592	51150.990695	33.260685
820.489815	51234.023332	33.265703
821.767171	51304.525852	33.270720
822.562836	51396.268265	33.275738
823.193915	51482.290559	33.280756
824.533330	51561.093540	33.285773
824.994321	51641.109678	33.290791
825.765210	51710.037578	33.295808
826.626832	51796.782097	33.300826
827.681648	51877.970289	33.305844
829.022994	51946.527427	33.310861
829.586553	52016.590921	33.315879
830.523115	52082.265364	33.320896
831.439800	52149.720014	33.325914
832.067996	52229.090435	33.330932
833.462512	52294.803226	33.335949
833.844307	52376.548941	33.340967
834.563096	52427.135779	33.345984
835.224018	52500.082873	33.351002
835.987444	52564.394831	33.356020
836.799372	52639.035334	33.361037
837.301388	52717.358092	33.366055
838.154251	52778.058675	33.371072
838.940420	52849.844755	33.376090
839.286051	52930.948587	33.381108
840.385594	53009.859229	33.386125
840.964893	53106.691421	33.391143
841.257656	53182.862309	33.396160
842.384847	53272.910868	33.401178
843.465105	53365.059886	33.406196
844.096468	53442.194261	33.411213
844.548629	53536.940661	33.416231
845.533463	53619.628102	33.421248
846.607335	53731.358003	33.426266
847.150844	53819.602129	33.431284
848.398516	53913.311732	33.436301
849.166406	54015.976798	33.441319
850.073581	54097.438361	33.446336
850.926190	54199.952108	33.451354
851.757789	54297.946755	33.456372
852.930914	54370.933505	33.461389
853.038689	54487.685748	33.466407
854.184354	54574.562537	33.471424
855.642708	54683.841421	33.476442
856.050003	54768.977535	33.481460
857.248054	54852.952888	33.486477
858.295885	54935.266997	33.491495
859.126969	55032.271403	33.496512
860.087232	55117.851427	33.501530
861.074176	55212.944419	33.506548
862.187143	55286.607285	33.511565
862.605626	55387.495457	33.516583
863.790681	55465.370996	33.521600
864.810364	55549.737796	33.526618
865.441545	55642.730569	33.531636
866.046964	55718.054234	33.536653
867.417538	55820.008553	33.541671
868.092668	55901.294156	33.546688
869.117742	55984.326859	33.551706
869.814101	56080.310275	33.556724
870.502600	56158.002635	33.561741
871.250542	56245.496785	33.566759
872.322572	56338.176711	33.571776
873.457530	56431.689931	33.576794
874.077847	56516.557214	33.581812
875.400103	56594.459925	33.586829
876.084605	56703.533128	33.591847
876.568376	56775.237614	33.596864
877.802758	56857.486500	33.601882
878.450103	56947.055062	33.606900
879.900492	57028.155991	33.611917
880.369044	57115.547223	33.616935
881.258703	57192.463784	33.621952
882.535447	57254.368264	33.626970
882.745529	57348.715217	33.631988
883.621848	57426.143131	33.637005
884.573131	57513.295271	33.642023
885.216840	57586.852655	33.647040
885.759121	57675.383919	33.652058
886.747724	57762.733341	33.657076
887.800150	57840.936832	33.662093
888.463089	57945.184385	33.667111
889.257457	58037.721333	33.672128
890.086936	58126.389000	33.677146
890.909781	58226.350757	33.682164
891.979846	58314.258085	33.687181
892.804189	58410.119626	33.692199
893.306367	58513.227859	33.697216
894.128786	58612.636126	33.702234
895.183107	58715.809159	33.707252
896.457270	58815.137154	33.712269
896.748347	58930.464575	33.717287
897.877669	59028.547597	33.722304
899.146382	59120.146252	33.727322
899.962817	59240.396090	33.732340
901.157547	59329.440765	33.737357
902.174761	59427.891029	33.742375
902.973817	59529.495870	33.747392
904.287702	59604.523761	33.752410
904.886456	59709.362900	33.757428
906.261152	59787.854838	33.762445
906.893382	59895.013446	33.767463
907.961265	59983.358418	33.772480
909.140156	60073.706830	33.777498
909.919188	60168.725860	33.782516
910.608703	60248.313861	33.787533
911.729585	60347.049276	33.792551
912.289414	60434.463716	33.797568
913.386386	60532.452459	33.802586
914.205143	60630.836461	33.807604
915.294401	60726.974049	33.812621
916.041631	60833.241970	33.817639
916.795569	60928.736157	33.822656
917.977650	61004.513716	33.827674
918.896548	61116.480432	33.832692
919.676775	61206.086278	33.837709
920.552623	61307.451752	33.842727
921.234837	61403.130273	33.847744
922.251048	61508.907691	33.852762
923.385315	61606.643513	33.857780
924.645284	61700.791761	33.862797
925.526085	61798.407875	33.867815
925.954126	61900.596157	33.872832
927.081831	61984.277238	33.877850
927.713206	62092.288471	33.882868
928.867421	62188.246379	33.887885
929.738035	62281.610074	33.892903
930.505449	62374.087548	33.897920
931.641168	62469.124622	33.902938
932.343199	62563.861727	33.907956
933.353482	62641.144731	33.912973
934.492146	62731.142888	33.917991
934.904414	62826.445289	33.923008
936.011552	62925.995365	33.928026
936.979181	63007.511789	33.933044
937.547938	63107.486372	33.938061
938.816588	63207.823794	33.943079
939.809293	63306.269886	33.948096
940.845078	63382.629768	33.953114
941.522006	63501.915416	33.958132
942.462732	63590.338629	33.963149
943.398354	63701.307492	33.968167
944.097835	63801.864939	33.973184
944.900085	63907.080347	33.978202
946.000817	64019.559565	33.983220
947.043432	64118.339832	33.988237
948.209002	64229.445721	33.993255
949.134956	64334.779606	33.998272
950.173278	64435.788616	34.003290
951.189170	64544.273714	34.008308
952.142789	64644.116188	34.013325
953.249728	64749.142497	34.018343
953.712298	64853.457115	34.023360
954.856282	64946.171434	34.028378
956.095733	65054.014340	34.033396
956.908383	65157.782246	34.038413
958.043892	65252.896453	34.043431
958.791479	65365.206091	34.048448
960.066053	65468.624265	34.053466
960.771253	65581.639882	34.058484
961.925884	65687.933372	34.063501
963.056357	65782.728870	34.068519
963.839630	65900.237636	34.073536
965.031078	65993.972767	34.078554
966.022498	66099.631263	34.083572
966.845936	66202.578785	34.088589
968.194300	66297.342159	34.093607
968.788848	66399.190143	34.098624
969.852569	66506.390131	34.103642
970.750456	66610.705050	34.108660
971.657329	66717.454249	34.113677
972.860665	66818.585381	34.118695
973.242830	66927.636450	34.123712
974.633395	67028.277760	34.128730
975.726969	67140.296357	34.133748
976.579745	67237.145690	34.138765
977.584860	67343.175214	34.143783
978.208095	67455.305212	34.148800
979.335352	67549.036016	34.153818
980.283735	67660.237391	34.158836
980.907278	67772.539739	34.163853
982.439756	67874.230484	34.168871
983.005824	67982.323286	34.173888
983.889167	68077.978001	34.178906
985.223755	68176.625297	34.183924
985.937665	68272.358465	34.188941
986.922826	68376.040443	34.193959
988.023474	68475.042345	34.198976
989.277871	68572.478833	34.203994
990.187830	68687.722743	34.209012
990.993303	68779.893415	34.214029
992.173367	68874.620393	34.219047
992.708082	68979.697620	34.224064
993.869544	69085.977132	34.229082
995.001001	69188.989453	34.234100
995.821586	69290.396542	34.239117
996.735603	69400.804678	34.244135
997.610571	69517.322602	34.249152
998.592178	69619.748213	34.254170
999.624899	69735.446299	34.259188
1000.513462	69851.761882	34.264205
1001.334366	69957.064183	34.269223
1002.441215	70082.658995	34.274240
1003.629316	70192.528877	34.279258
1004.714059	70304.753482	34.284276
1005.552893	70431.682042	34.289293
1006.992720	70533.527773	34.294311
1007.687546	70654.674365	34.299328
1008.516416	70770.815349	34.304346
1009.540289	70885.239038	34.309364
1010.793990	71001.345389	34.314381
1012.338937	71109.394527	34.319399
1013.423618	71238.494258	34.324416
1014.352648	71341.170996	34.329434
1015.701078	71455.761192	34.334452
1016.302539	71557.998336	34.339469
1017.700660	71667.685090	34.344487
1018.604238	71779.352990	34.349504
1019.706746	71879.060516	34.354522
1020.617446	71981.813005	34.359540
1021.230297	72104.479036	34.364557
1022.812134	72216.079415	34.369575
1023.425502	72327.486963	34.374592
1024.491455	72440.680835	34.379610
1025.546492	72552.531200	34.384628
1026.518967	72658.032335	34.389645
1028.030281	72767.966252	34.394663
1028.599278	72889.247656	34.399680
1029.646021	72994.587113	34.404698
1030.703744	73101.201799	34.409716
1032.051166	73224.383464	34.414733
1033.199198	73321.342262	34.419751
1033.846598	73433.117092	34.424768
1035.048072	73538.624385	34.429786
1036.391829	73653.853619	34.434804
1037.515605	73758.616147	34.439821
1038.487995	73871.182175	34.444839
1039.424602	73974.402143	34.449856
1040.216276	74052.185610	34.454874
1041.473656	74148.385369	34.459892
1041.855247	74242.626910	34.464909
1043.333112	74348.593741	34.469927
1043.934392	74456.261448	34.474944
1044.936082	74556.611410	34.479962
1046.313366	74662.564306	34.484980
1047.318299	74761.733052	34.489997
1048.266033	74869.802868	34.495015
1049.281116	74981.395150	34.500032
1050.148325	75076.928373	34.505050
1051.487829	75199.472560	34.510068
1051.857845	75298.340499	34.515085
1053.380553	75413.709388	34.520103
1054.168740	75527.780173	34.525120
1054.955848	75637.320547	34.530138
1056.379545	75748.434986	34.535156
1057.288356	75875.462974	34.540173
1058.637205	75997.549188	34.545191
1059.201252	76119.773615	34.550208
1060.921110	76232.891247	34.555226
1061.919559	76344.537964	34.560244
1062.658485	76468.512580	34.565261
1063.810340	76580.490115	34.570279
1064.849751	76710.984895	34.575296
1065.695381	76827.038366	34.580314
1066.990126	76947.280818	34.585332
1068.188950	77067.178991	34.590349
1069.529068	77198.355892	34.595367
1070.195397	77321.272833	34.600384
1071.166243	77436.583044	34.605402
1072.564616	77577.094473	34.610420
1073.362266	77694.310824	34.615437
1074.676468	77803.102788	34.620455
1075.703187	77923.336762	34.625472
1076.941862	78057.076141	34.630490
1078.242912	78180.914901	34.635508
1078.996097	78306.288957	34.640525
1079.777783	78418.740006	34.645543
1081.164868	78542.548313	34.650560
1082.409752	78676.227550	34.655578
1083.358829	78800.593776	34.660596
1084.371150	78932.876884	34.665613
1085.886802	79052.142186	34.670631
1087.141501	79161.146790	34.675648
1087.899225	79297.638149	34.680666
1089.120832	79397.534628	34.685684
1089.795015	79532.188817	34.690701
1091.376072	79648.786082	34.695719
1091.949254	79784.589435	34.700736
1092.948605	79905.762257	34.705754
1094.125545	80024.631964	34.710772
1095.302483	80155.872745	34.715789
1096.642796	80266.835455	34.720807
1097.823721	80390.219925	34.725824
1098.691607	80511.815450	34.730842
1099.973990	80614.274576	34.735860
1100.805997	80721.711148	34.740877
1102.058327	80828.980286	34.745895
1103.127158	80938.257744	34.750912
1104.181641	81055.085780	34.755930
1105.668627	81168.135019	34.760948
1106.397611	81290.307169	34.765965
1107.429306	81405.269654	34.770983
1108.704050	81516.970148	34.776000
1109.418870	81634.076718	34.781018
1110.443943	81759.112445	34.786036
1111.282406	81876.023707	34.791053
1112.641655	82004.263394	34.796071
1113.465988	82138.284799	34.801088
1114.298057	82263.063448	34.806106
1115.608278	82389.675973	34.811124
1117.139533	82532.210385	34.816141
1118.466910	82660.667798	34.821159
1119.740721	82783.223545	34.826176
1120.604835	82912.015378	34.831194
1122.017366	83028.241207	34.836212
1122.947018	83152.257328	34.841229
1124.153980	83287.230442	34.846247
1125.357374	83417.128355	34.851264
1126.101619	83550.337023	34.856282
1127.861101	83665.986474	34.861300
1128.992665	83794.829702	34.866317
1129.868561	83930.580333	34.871335
1131.177776	84054.648895	34.876352
1132.254171	84183.123936	34.881370
1133.970633	84294.908110	34.886388
1134.937400	84423.364117	34.891405
1136.271027	84539.560278	34.896423
1137.649299	84664.727875	34.901440
1138.550064	84780.810852	34.906458
1139.662081	84899.889364	34.911476
1140.746595	85024.827619	34.916493
1141.743258	85149.458128	34.921511
1142.950949	85268.789050	34.926528
1143.845606	85391.097825	34.931546
1144.997771	85510.578036	34.936564
1146.048543	85650.883224	34.941581
1146.994399	85772.256607	34.946599
1148.284044	85907.106867	34.951616
1149.113406	86035.126604	34.956634
1150.690543	86171.798069	34.961652
1151.628683	86304.917365	34.966669
1152.902103	86433.539111	34.971687
1154.214525	86557.451101	34.976704
1155.376926	86688.754035	34.981722
1156.444878	86813.673818	34.986740
1157.596345	86952.928252	34.991757
1158.815422	87075.018054	34.996775
1160.268244	87192.031782	35.001792
1160.691625	87313.161884	35.006810
1162.139623	87418.365793	35.011828
1163.428608	87534.692917	35.016845
1164.586522	87655.012577	35.021863
1165.706224	87763.432061	35.026880
1166.496469	87897.773575	35.031898
1167.671550	87996.453689	35.036916
1168.987732	88144.567789	35.041933
1170.104033	88264.378951	35.046951
1171.360347	88391.408994	35.051968
1171.947687	88513.183752	35.056986
1173.056261	88645.980617	35.062004
1174.428335	88786.735850	35.067021
1175.238136	88915.635907	35.072039
1176.753553	89047.472577	35.077056
1177.656473	89189.165065	35.082074
1178.839358	89332.413890	35.087092
1180.082287	89482.951874	35.092109
1181.300688	89621.858781	35.097127
1182.951987	89747.518606	35.102144
1183.807113	89902.377189	35.107162
1185.195063	90029.769032	35.112180
1186.201537	90175.941561	35.117197
1187.294229	90318.174079	35.122215
1189.039984	90456.566099	35.127232
1189.943162	90601.100973	35.132250
1191.245585	90732.121647	35.137268
1192.088706	90882.397698	35.142285
1193.487789	91023.346531	35.147303
1195.110060	91156.159268	35.152320
1195.973254	91306.346497	35.157338
1197.216877	91448.688862	35.162356
1198.811103	91583.899297	35.167373
1199.840819	91719.137081	35.172391
1201.046930	91865.845718	35.177408
1202.061760	92006.982142	35.182426
1203.440915	92145.544330	35.187444
1204.430218	92299.430865	35.192461
1205.756408	92436.086920	35.197479
1207.243959	92577.967730	35.202496
1208.285854	92723.911272	35.207514
1209.493215	92869.475276	35.212532
1211.064984	93004.343818	35.217549
1212.273366	93145.311276	35.222567
1213.624403	93280.298822	35.227584
1214.811016	93417.824366	35.232602
1216.099705	93552.753911	35.237620
1217.037022	93686.057670	35.242637
1218.638789	93831.868894	35.247655
1219.786216	93960.232589	35.252672
1220.645738	94104.519073	35.257690
1221.843003	94240.226355	35.262708
1223.224311	94378.960315	35.267725
1223.925538	94506.607443	35.272743
1225.331219	94646.155158	35.277760
1226.381062	94777.208379	35.282778
1227.830828	94908.110227	35.287796
1228.862553	95036.359354	35.292813
1230.281593	95166.261849	35.297831
1231.702007	95282.362541	35.302848
1232.548221	95420.365725	35.307866
1234.135824	95548.383916	35.312884
1235.659542	95669.992459	35.317901
1236.519653	95801.202026	35.322919
1238.005723	95919.933395	35.327936
1238.709530	96059.879845	35.332954
1240.268072	96203.613266	35.337972
1241.186442	96339.333332	35.342989
1242.591754	96474.179735	35.348007
1243.824217	96612.527354	35.353024
1244.638779	96742.364269	35.358042
1246.019861	96893.582277	35.363060
1247.312827	97039.229416	35.368077
1248.491277	97190.247560	35.373095
1249.699899	97336.371824	35.378112
1250.897053	97490.615317	35.383130
1252.127662	97640.559047	35.388148
1253.361299	97787.169354	35.393165
1254.374731	97937.288747	35.398183
1255.815998	98095.793087	35.403200
1257.002878	98249.005841	35.408218
1258.204076	98402.799379	35.413236
1259.931115	98547.590051	35.418253
1261.146206	98710.057023	35.423271
1262.355392	98851.192990	35.428288
1263.560621	99022.457640	35.433306
1265.045081	99169.479819	35.438324
1266.216585	99315.831456	35.443341
1267.510365	99477.272769	35.448359
1269.163338	99615.761597	35.453376
1270.753666	99765.725362	35.458394
1272.163605	99922.526456	35.463412
1273.530528	100062.284532	35.468429
1274.732379	100210.395914	35.473447
1276.305470	100337.734794	35.478464
1277.458621	100489.797402	35.483482
1278.662307	100624.675096	35.488500
1279.821692	100774.131850	35.493517
1280.982752	100912.409308	35.498535
1282.486953	101056.435032	35.503552
1283.495714	101216.484921	35.508570
1284.584135	101348.613850	35.513588
1285.902450	101503.485131	35.518605
1286.965183	101650.450977	35.523623
1288.361044	101789.291104	35.528640
1289.696304	101959.367340	35.533658
1291.233993	102104.767289	35.538676
1292.494719	102249.908457	35.543693
1293.727584	102396.465991	35.548711
1295.275868	102518.467725	35.553728
1296.509264	102655.605096	35.558746
1297.604586	102784.260907	35.563764
1298.972680	102915.259588	35.568781
1299.896471	103052.739575	35.573799
1301.136999	103177.286780	35.578816
1302.396891	103332.508531	35.583834
1303.443024	103485.056989	35.588852
1304.822012	103616.969063	35.593869
1305.907210	103766.646629	35.598887
1307.270209	103904.270602	35.603904
1308.329154	104055.409597	35.608922
1309.639711	104223.050948	35.613940
1311.246555	104363.638315	35.618957
1312.224095	104521.266815	35.623975
1313.600775	104682.806980	35.628992
1315.051653	104847.000610	35.634010
1316.195679	104997.379053	35.639028
1317.840073	105151.102493	35.644045
1319.046458	105320.856502	35.649063
1320.354908	105475.167019	35.654080
1321.778687	105634.149531	35.659098
1322.892830	105801.447238	35.664116
1324.430928	105969.134380	35.669133
1325.665669	106141.186964	35.674151
1327.242519	106300.320459	35.679168
1328.396520	106462.983970	35.684186
1329.776210	106619.625821	35.689204
1331.495277	106774.316150	35.694221
1332.573822	106952.386327	35.699239
1333.956464	107113.290168	35.704256
1335.472232	107274.813138	35.709274
1336.568264	107429.537108	35.714292
1338.140241	107594.413910	35.719309
1339.323799	107754.524603	35.724327
1341.246983	107911.968219	35.729344
1342.438507	108075.522741	35.734362
1343.655897	108233.314813	35.739380
1345.314195	108388.189738	35.744397
1346.601942	108552.649913	35.749415
1348.186159	108699.798068	35.754432
1349.823083	108854.976851	35.759450
1350.913441	109011.072633	35.764468
1352.570395	109161.946298	35.769485
1353.534959	109314.393028	35.774503
1355.044979	109470.146565	35.779520
1356.572276	109617.695423	35.784538
1357.890405	109780.855222	35.789556
1359.749434	109930.752116	35.794573
1360.858342	110076.825853	35.799591
1362.120481	110227.123255	35.804608
1363.381263	110378.877607	35.809626
1364.553938	110519.348469	35.814644
1366.070938	110680.203986	35.819661
1367.287573	110831.461782	35.824679
1368.650839	110972.822760	35.829696
1370.051836	111103.449536	35.834714
1370.835052	111241.891266	35.839732
1372.227628	111376.033888	35.844749
1373.689993	111547.411357	35.849767
1375.063626	111668.841783	35.854784
1375.837441	111823.435976	35.859802
1377.015528	111981.264826	35.864820
1378.612070	112130.140762	35.869837
1379.873708	112293.857950	35.874855
1381.460950	112460.594593	35.879872
1382.600550	112612.457920	35.884890
1383.719860	112777.751817	35.889908
1385.450467	112955.717825	35.894925
1386.880886	113118.185549	35.899943
1387.979681	113284.916726	35.904960
1389.551955	113449.117572	35.909978
1390.652433	113621.383501	35.914996
1392.212063	113791.178390	35.920013
1393.728712	113961.139526	35.925031
1395.030325	114134.472204	35.930048
1396.613113	114310.116384	35.935066
1397.742995	114476.306124	35.940084
1399.449241	114656.206301	35.945101
1400.941535	114822.973809	35.950119
1402.503444	114998.182963	35.955136
1404.385332	115157.179866	35.960154
1405.560748	115332.484420	35.965172
1407.182581	115488.175704	35.970189
1408.486760	115658.460634	35.975207
1410.287307	115825.084482	35.980224
1411.639427	115985.304036	35.985242
1412.709422	116160.118259	35.990260
1414.540714	116319.871250	35.995277
1415.594278	116486.193964	36.000295
1417.073355	116652.241213	36.005312
1418.682460	116827.449189	36.010330
1420.030444	116998.413582	36.015348
1421.998890	117152.958349	36.020365
1423.415625	117311.434867	36.025383
1424.571591	117473.777977	36.030400
1426.179769	117641.254704	36.035418
1427.133577	117804.106890	36.040436
1428.724873	117969.973917	36.045453
1430.180760	118150.970666	36.050471
1431.547191	118299.134486	36.055488
1433.039301	118461.208815	36.060506
1434.759073	118641.179339	36.065524
1436.122598	118803.111628	36.070541
1437.527041	118974.270157	36.075559
1439.155967	119129.146708	36.080576
1440.692034	119311.443211	36.085594
1441.920245	119479.745761	36.090612
1443.536135	119620.405879	36.095629
1444.819476	119798.718857	36.100647
1445.787264	119941.858195	36.105664
1447.718850	120078.570111	36.110682
1448.719500	120256.785512	36.115700
1450.067804	120391.242551	36.120717
1450.935243	120553.980121	36.125735
1452.724930	120705.186864	36.130752
1454.127330	120857.443852	36.135770
1455.423025	121038.885134	36.140788
1457.155255	121181.263903	36.145805
1458.473961	121351.419515	36.150823
1459.576405	121526.638514	36.155840
1461.219921	121701.962678	36.160858
1462.839775	121854.342876	36.165876
1463.900610	122026.405576	36.170893
1465.401528	122215.991316	36.175911
1466.641983	122389.661642	36.180928
1468.474574	122569.103049	36.185946
1469.719714	122743.154909	36.190964
1471.032226	122927.861522	36.195981
1472.949500	123107.293119	36.200999
1474.193116	123287.440919	36.206016
1475.153082	123484.911051	36.211034
1477.374702	123670.909602	36.216052
1479.138271	123841.833820	36.221069
1480.700030	124035.526634	36.226087
1482.527285	124202.934567	36.231104
1483.870720	124373.827615	36.236122
1485.311326	124547.404220	36.241140
1486.898760	124728.330412	36.246157
1488.396059	124904.015590	36.251175
1489.566134	125080.627894	36.256192
1491.791817	125249.714364	36.261210
1493.644840	125422.927099	36.266228
1495.015719	125588.972189	36.271245
1496.561205	125775.422105	36.276263
1497.995409	125940.344613	36.281280
1499.816143	126097.581207	36.286298
1500.748831	126275.379064	36.291316
1502.158507	126460.195887	36.296333
1504.251473	126621.952434	36.301351
1505.608975	126787.386298	36.306368
1507.388221	126949.422649	36.311386
1508.972604	127123.018282	36.316404
1510.120642	127285.625611	36.321421
1511.965882	127456.800432	36.326439
1513.213660	127629.401352	36.331456
1515.023888	127793.603961	36.336474
1516.208557	127964.608216	36.341492
1517.306308	128124.834298	36.346509
1519.221406	128315.473942	36.351527
1520.278637	128504.300318	36.356544
1521.979551	128642.226472	36.361562
1523.087392	128836.190341	36.366580
1524.517197	129023.124183	36.371597
1526.083642	129177.771207	36.376615
1527.422707	129378.948458	36.381632
1529.450866	129517.485753	36.386650
1530.538262	129721.467210	36.391668
1532.066468	129852.383084	36.396685
1533.406285	130044.468923	36.401703
1534.878787	130195.399256	36.406720
1536.395455	130356.889261	36.411738
1537.714009	130555.861221	36.416756
1539.276303	130730.065816	36.421773
1540.583946	130907.200521	36.426791
1542.059377	131073.034067	36.431808
1543.661489	131289.855159	36.436826
1545.241088	131476.376237	36.441844
1546.699997	131661.752132	36.446861
1548.272921	131842.334700	36.451879
1549.654655	132051.126142	36.456896
1551.549667	132227.732411	36.461914
1552.752795	132415.320416	36.466932
1554.099282	132626.161543	36.471949
1555.982910	132821.360120	36.476967
1557.594526	133010.432910	36.481984
1559.343762	133209.785959	36.487002
1560.898216	133428.518870	36.492020
1562.518363	133608.484340	36.497037
1564.131313	133798.765834	36.502055
1565.877181	134000.887104	36.507072
1567.463367	134205.138492	36.512090
1569.323585	134378.481941	36.517108
1570.879277	134615.989054	36.522125
1572.612433	134773.060408	36.527143
1573.947850	135002.255589	36.532160
1576.389934	135152.564135	36.537178
1577.353050	135368.250671	36.542196
1579.074185	135549.872180	36.547213
1581.089371	135718.637435	36.552231
1582.363536	135939.131917	36.557248
1584.194608	136125.985528	36.562266
1585.969429	136311.328690	36.567284
1587.387621	136489.101359	36.572301
1588.757973	136691.655909	36.577319
1590.526574	136874.127157	36.582336
1592.230606	137052.187317	36.587354
1593.786243	137251.801785	36.592372
1595.058584	137434.976283	36.597389
1596.999003	137641.172430	36.602407
1598.585290	137830.394819	36.607424
1600.081061	138001.194625	36.612442
1601.576789	138204.943572	36.617460
1603.077548	138407.299155	36.622477
1605.058752	138566.771988	36.627495
1606.323953	138786.364200	36.632512
1608.214085	138963.012365	36.637530
1609.883318	139152.635569	36.642548
1611.411775	139349.138358	36.647565
1613.063014	139528.273690	36.652583
1614.464751	139712.861104	36.657600
1615.864882	139884.409307	36.662618
1617.514049	140063.674912	36.667636
1619.108336	140238.083785	36.672653
1620.495409	140413.996690	36.677671
1621.838271	140607.318208	36.682688
1623.592173	140776.204606	36.687706
1625.451975	140960.143967	36.692724
1626.746114	141151.727771	36.697741
1628.413608	141346.231811	36.702759
1629.926694	141529.177792	36.707776
1631.861900	141711.867728	36.712794
1633.295493	141908.668478	36.717812
1634.629843	142106.424144	36.722829
1636.211259	142295.713579	36.727847
1637.557089	142505.890633	36.732864
1639.284380	142697.453423	36.737882
1641.233873	142895.927665	36.742900
1642.551602	143109.700175	36.747917
1644.484544	143311.006137	36.752935
1646.346352	143519.054931	36.757952
1648.138201	143715.316113	36.762970
1649.627752	143921.272055	36.767988
1651.827069	144117.914707	36.773005
1653.799652	144310.234448	36.778023
1655.158376	144523.503269	36.783040
1657.193511	144714.776241	36.788058
1658.956470	144896.752021	36.793076
1660.177048	145127.158411	36.798093
1662.500572	145290.947209	36.803111
1663.921059	145484.591421	36.808128
1665.350223	145700.468262	36.813146
1667.421070	145885.645851	36.818164
1668.501718	146085.685542	36.823181
1670.806867	146288.713651	36.828199
1672.164570	146477.772689	36.833216
1673.594402	146688.446471	36.838234
1675.514225	146878.736939	36.843252
1676.970141	147079.103630	36.848269
1678.881252	147304.383959	36.853287
1680.605088	147489.042998	36.858304
1682.172441	147689.383180	36.863322
1683.936829	147887.107356	36.868340
1686.072567	148107.806905	36.873357
1687.836838	148281.600410	36.878375
1688.661711	148524.555504	36.883392
1690.610279	148690.880793	36.888410
1692.523605	148924.298001	36.893428
1693.928346	149118.765604	36.898445
1695.705679	149312.642785	36.903463
1697.264145	149542.875547	36.908480
1698.763797	149712.738252	36.913498
1700.693666	149949.823957	36.918516
1702.253457	150148.367883	36.923533
1704.363322	150347.332771	36.928551
1705.961092	150538.659654	36.933568
1707.706703	150730.610741	36.938586
1709.480512	150904.074601	36.943604
1710.849403	151078.706638	36.948621
1712.628970	151265.229462	36.953639
1714.168055	151464.976422	36.958656
1715.723108	151651.727270	36.963674
1717.437280	151828.235516	36.968692
1719.178000	152054.526969	36.973709
1721.079797	152214.881088	36.978727
1722.610432	152429.455919	36.983744
1724.093203	152647.703753	36.988762
1725.662291	152830.135788	36.993780
1727.263308	153041.787410	36.998797
1728.971421	153247.578609	37.003815
1730.793592	153464.890443	37.008832
1732.360095	153683.017689	37.013850
1734.342738	153893.080023	37.018868
1735.913568	154107.824147	37.023885
1737.974941	154315.353559	37.028903
1739.661637	154534.583021	37.033920
1741.348323	154754.485905	37.038938
1743.500207	154970.854965	37.043956
1745.227806	155171.050745	37.048973
1746.442637	155399.122080	37.053991
1748.798686	155599.220614	37.059008
1750.044215	155843.519635	37.064026
1752.183162	156049.310329	37.069044
1753.781263	156264.672479	37.074061
1755.573187	156478.103266	37.079079
1757.775576	156710.806843	37.084096
1759.187995	156934.520627	37.089114
1761.616025	157150.060906	37.094132
1762.764613	157364.550364	37.099149
1764.837389	157603.899548	37.104167
1766.823249	157814.226605	37.109184
1768.740900	158015.600844	37.114202
1770.538066	158236.320190	37.119220
1772.183299	158456.988983	37.124237
1774.092060	158681.269318	37.129255
1776.336393	158881.341356	37.134272
1777.836434	159102.366994	37.139290
1779.898325	159303.345387	37.144308
1781.068661	159542.267915	37.149325
1783.395059	159732.415426	37.154343
1785.408430	159944.970158	37.159360
1786.927309	160143.833104	37.164378
1789.070028	160365.982054	37.169396
1790.456848	160581.861104	37.174413
1792.416366	160776.231931	37.179431
1794.099277	160984.964940	37.184448
1795.523767	161222.704506	37.189466
1797.793482	161426.502657	37.194484
1799.450182	161626.632881	37.199501
1800.934842	161852.154774	37.204519
1803.166057	162036.825968	37.209536
1804.522408	162217.781756	37.214554
1806.732744	162414.315652	37.219572
1808.026775	162618.973004	37.224589
1809.970756	162781.424241	37.229607
1811.484282	163003.765620	37.234624
1812.896360	163207.228142	37.239642
1814.904068	163388.733197	37.244660
1816.589102	163613.346567	37.249677
1818.456919	163808.813719	37.254695
1820.031006	164020.904422	37.259712
1821.536992	164241.821477	37.264730
1823.468236	164460.529010	37.269748
1825.236357	164672.453187	37.274765
1826.973895	164884.180521	37.279783
1829.179971	165130.002051	37.284800
1830.757600	165354.326101	37.289818
1833.009676	165567.814701	37.294836
1834.578310	165791.559422	37.299853
1836.244149	166017.725212	37.304871
1838.385915	166251.934045	37.309888
1840.049348	166489.898422	37.314906
1842.359812	166715.788564	37.319924
1844.117470	166935.286619	37.324941
1845.834195	167163.429893	37.329959
1847.951396	167386.044381	37.334976
1849.854833	167618.320980	37.339994
1851.404518	167845.023609	37.345012
1853.585340	168074.493945	37.350029
1855.608404	168303.914613	37.355047
1857.607251	168537.158374	37.360064
1859.311064	168769.004425	37.365082
1861.521142	168994.112388	37.370100
1863.162440	169213.921204	37.375117
1865.001320	169458.649782	37.380135
1867.147998	169671.886686	37.385152
1868.290250	169933.573616	37.390170
1871.043464	170136.099996	37.395188
1872.800685	170380.492241	37.400205
1874.755989	170585.709910	37.405223
1876.275820	170845.085223	37.410240
1878.290720	171051.412150	37.415258
1880.296869	171292.168160	37.420276
1882.404891	171507.222567	37.425293
1883.939917	171756.770746	37.430311
1885.891281	171970.089353	37.435328
1887.732598	172203.570551	37.440346
1889.667997	172434.336256	37.445364
1891.666696	172670.509874	37.450381
1893.885206	172893.038643	37.455399
1895.653619	173143.966637	37.460416
1897.527631	173340.560180	37.465434
1899.683488	173584.858383	37.470452
1901.303096	173808.489498	37.475469
1903.189757	174027.677539	37.480487
1905.423026	174211.380428	37.485504
1907.050547	174449.234603	37.490522
1909.019529	174620.257421	37.495540
1910.935351	174838.316217	37.500557
1912.351867	175046.141700	37.505575
1914.336277	175239.276436	37.510592
1915.794219	175476.985974	37.515610
1918.071819	175678.373015	37.520628
1919.799008	175895.351048	37.525645
1921.313385	176096.125482	37.530663
1923.610691	176329.951619	37.535680
1925.439822	176541.740845	37.540698
1927.462202	176772.745995	37.545716
1929.454829	176995.434737	37.550733
1931.155544	177258.984122	37.555751
1933.350108	177457.335585	37.560768
1935.144305	177692.441859	37.565786
1937.220029	177924.903967	37.570804
1939.168344	178148.468647	37.575821
1940.994463	178392.518125	37.580839
1943.102428	178612.329957	37.585856
1944.860476	178854.565984	37.590874
1946.886926	179083.616808	37.595892
1949.067329	179317.516379	37.600909
1951.306071	179550.101185	37.605927
1953.208835	179769.672497	37.610944
1954.856545	180020.179567	37.615962
1956.703334	180255.025381	37.620980
1958.866580	180494.668960	37.625997
1960.718594	180726.040108	37.631015
1962.981524	180972.027102	37.636032
1965.057939	181203.530154	37.641050
1967.053426	181439.589582	37.646068
1969.015999	181683.915429	37.651085
1970.850827	181923.530263	37.656103
1973.084125	182148.796311	37.661120
1974.965944	182401.234057	37.666138
1977.165915	182629.235848	37.671156
1979.355406	182859.499020	37.676173
1981.228348	183114.962122	37.681191
1983.636501	183332.974109	37.686208
1985.427940	183566.539718	37.691226
1987.203416	183792.001053	37.696244
1989.401196	184051.630654	37.701261
1991.426959	184264.797380	37.706279
1993.341960	184501.583938	37.711296
1995.085334	184753.473409	37.716314
1997.288744	184967.478146	37.721332
1999.374675	185207.819605	37.726349
2001.153506	185457.106141	37.731367
2003.877961	185668.417579	37.736384
2005.875727	185908.814829	37.741402
2007.776547	186146.906592	37.746420
2009.851901	186355.037699	37.751437
2011.935155	186579.233308	37.756455
2014.230247	186778.525023	37.761472
2015.788888	186989.253524	37.766490
2017.627584	187177.427223	37.771508
2019.732166	187381.941829	37.776525
2021.300525	187586.136354	37.781543
2023.748227	187797.006656	37.786560
2025.364541	188004.494755	37.791578
2027.335395	188210.937716	37.796596
2029.307060	188419.310333	37.801613
2031.139008	188634.177940	37.806631
2033.266895	188844.151982	37.811648
2034.925135	189079.733964	37.816666
2037.229205	189304.618367	37.821684
2039.249344	189525.614922	37.826701
2041.166184	189764.471441	37.831719
2043.336732	190002.121398	37.836736
2045.095845	190229.380920	37.841754
2047.406180	190449.409334	37.846772
2049.682027	190677.591553	37.851789
2051.329446	190937.994458	37.856807
2053.646703	191147.085683	37.861824
2055.823573	191383.573956	37.866842
2057.840374	191616.306931	37.871860
2059.796187	191863.112148	37.876877
2062.189052	192104.696772	37.881895
2064.618241	192318.064821	37.886912
2066.673666	192562.167291	37.891930
2068.441575	192784.069124	37.896948
2070.568542	193028.124488	37.901965
2072.520065	193264.936834	37.906983
2075.064008	193506.314022	37.912000
2077.011726	193737.798903	37.917018
2079.346361	193975.404182	37.922036
2081.742097	194218.800890	37.927053
2083.903559	194439.556233	37.932071
2086.125957	194660.125198	37.937088
2088.351824	194912.829754	37.942106
2090.196986	195125.172974	37.947124
2092.488508	195338.867749	37.952141
2094.301827	195572.793838	37.957159
2096.735342	195806.673382	37.962176
2098.839132	196044.883477	37.967194
2100.717455	196274.423764	37.972212
2103.049828	196486.873058	37.977229
2105.052190	196725.216630	37.982247
2106.819760	196942.859614	37.987264
2108.885011	197178.111111	37.992282
2111.301924	197404.588323	37.997300
2113.529605	197635.932302	38.002317
2116.006987	197870.499629	38.007335
2118.227605	198098.978308	38.012352
2120.044970	198325.478462	38.017370
2122.376496	198540.995162	38.022388
2124.516899	198756.124206	38.027405
2126.774555	198984.105834	38.032423
2128.921852	199172.720607	38.037440
2131.421233	199368.185032	38.042458
2133.155393	199562.324583	38.047476
2135.049620	199751.121165	38.052493
2136.748689	199944.975734	38.057511
2138.974633	200131.702875	38.062528
2140.928096	200357.238107	38.067546
2142.861183	200556.426867	38.072564
2145.285619	200758.787836	38.077581
2146.965142	200966.281484	38.082599
2148.655164	201179.689254	38.087616
2150.922436	201411.182931	38.092634
2153.201662	201639.565846	38.097652
2155.606558	201852.532818	38.102669
2157.406416	202077.744103	38.107687
2159.653250	202303.088500	38.112704
2161.692172	202534.724656	38.117722
2163.554655	202773.510811	38.122740
2165.960306	203001.193832	38.127757
2167.957176	203231.950998	38.132775
2169.683520	203490.995397	38.137792
2172.416056	203712.320703	38.142810
2174.253061	203970.029598	38.147828
2176.768146	204232.696946	38.152845
2178.902049	204460.314699	38.157863
2181.115351	204699.688032	38.162880
2183.653534	204948.112418	38.167898
2185.729334	205202.920147	38.172916
2188.697622	205420.000253	38.177933
2190.814761	205692.004062	38.182951
2193.049905	205901.712704	38.187968
2195.648459	206159.907232	38.192986
2197.886498	206384.037806	38.198004
2200.116181	206609.681188	38.203021
2202.160526	206859.004477	38.208039
2204.525259	207080.667586	38.213056
2206.971087	207309.681466	38.218074
2209.146972	207541.100221	38.223092
2211.342929	207785.757145	38.228109
2213.419474	208010.236831	38.233127
2215.622999	208236.690281	38.238144
2217.911410	208496.518273	38.243162
2220.412125	208692.585878	38.248180
2222.612849	208968.933012	38.253197
2224.417512	209178.365977	38.258215
2226.646176	209431.796513	38.263232
2229.386839	209643.266155	38.268250
2231.273947	209886.761781	38.273268
2233.463943	210133.561831	38.278285
2235.738777	210355.276534	38.283303
2237.773516	210595.120716	38.288320
2240.133185	210843.521646	38.293338
2242.289419	211068.202972	38.298356
2244.675701	211331.226551	38.303373
2246.645001	211534.014367	38.308391
2248.801131	211781.448325	38.313408
2250.912611	211958.290929	38.318426
2252.523374	212220.412828	38.323444
2254.989774	212404.703419	38.328461
2257.434200	212651.637979	38.333479
2259.016442	212876.111989	38.338496
2261.418278	213097.981153	38.343514
2263.609318	213336.515880	38.348532
2265.760217	213563.657053	38.353549
2267.669023	213814.984814	38.358567
2269.802383	214060.704446	38.363584
2272.452458	214301.163129	38.368602
2274.297592	214559.397683	38.373620
2276.718690	214806.102816	38.378637
2278.883652	215059.629157	38.383655
2281.151467	215322.497160	38.388672
2283.514057	215578.292106	38.393690
2285.605961	215837.381159	38.398708
2287.965160	216094.702125	38.403725
2290.094824	216365.861312	38.408743
2292.716356	216637.743445	38.413760
2295.318561	216904.716213	38.418778
2297.546544	217177.907112	38.423796
2300.038046	217440.138326	38.428813
2302.545132	217708.119576	38.433831
2304.585885	217972.277939	38.438848
2307.112691	218241.680106	38.443866
2309.440273	218505.756887	38.448884
2312.022544	218760.449482	38.453901
2314.045499	219039.342812	38.458919
2316.616021	219298.889341	38.463936
2319.614198	219570.608765	38.468954
2321.745679	219842.949102	38.473972
2324.043882	220087.749732	38.478989
2326.582568	220352.206082	38.484007
2328.996094	220618.130686	38.489024
2331.535436	220879.249497	38.494042
2333.427942	221148.077354	38.499060
2336.204485	221411.483993	38.504077
2338.397464	221672.736669	38.509095
2340.841419	221932.795007	38.514112
2343.375647	222187.684819	38.519130
2345.211548	222459.014980	38.524148
2347.463336	222723.042653	38.529165
2349.924446	222977.324509	38.534183
2351.997505	223273.506902	38.539200
2354.458165	223577.856969	38.544218
2356.824409	223858.872344	38.549236
2359.168576	224127.892972	38.554253
2361.707898	224404.299009	38.559271
2363.731840	224681.054361	38.564288
2366.503287	224946.327683	38.569306
2368.867817	225223.424540	38.574324
2370.927762	225486.336363	38.579341
2373.352307	225758.676545	38.584359
2375.317496	226006.266035	38.589376
2377.933445	226260.597302	38.594394
2379.685224	226509.263365	38.599412
2381.781160	226752.834498	38.604429
2384.059435	227017.633994	38.609447
2386.426313	227286.686842	38.614464
2389.076959	227538.680052	38.619482
2391.097258	227816.017921	38.624500
2393.316083	228100.055278	38.629517
2395.775366	228358.455754	38.634535
2398.042047	228640.582568	38.639552
2400.243239	228922.212746	38.644570
2402.442637	229214.104412	38.649588
2405.031409	229499.230553	38.654605
2407.204940	229786.785351	38.659623
2409.419636	230091.858497	38.664640
2412.263972	230390.407406	38.669658
2414.880253	230687.799784	38.674676
2417.098852	230984.672035	38.679693
2419.717931	231277.976934	38.684711
2421.768904	231581.328614	38.689728
2424.585359	231896.344401	38.694746
2427.261651	232197.389385	38.699764
2429.635734	232496.680000	38.704781
2432.234124	232791.161227	38.709799
2434.433478	233110.799685	38.714816
2437.140591	233406.637057	38.719834
2439.436231	233728.370328	38.724852
2441.779274	234023.886316	38.729869
2444.470070	234328.466016	38.734887
2446.926880	234653.884904	38.739904
2449.499218	234968.416058	38.744922
2452.520937	235262.228067	38.749940
2455.364974	235568.311159	38.754957
2458.164513	235870.160666	38.759975
2459.770769	236188.175925	38.764992
2462.505617	236474.010917	38.770010
2465.121289	236779.524230	38.775028
2467.492286	237080.835603	38.780045
2470.012948	237383.825839	38.785063
2472.834407	237692.890418	38.790080
2475.566699	237987.390955	38.795098
2477.912038	238286.068278	38.800116
2480.378636	238584.549403	38.805133
2482.936879	238879.664109	38.810151
2485.387613	239179.241520	38.815168
2487.585453	239485.133463	38.820186
2490.338386	239783.166022	38.825204
2492.593342	240105.001449	38.830221
2495.191138	240393.611556	38.835239
2497.815885	240693.266965	38.840256
2500.196332	241004.290140	38.845274
2502.678762	241305.036452	38.850292
2505.221753	241607.094719	38.855309
2507.827545	241902.082614	38.860327
2509.839791	242177.073903	38.865344
2512.371396	242440.426488	38.870362
2515.015254	242726.647331	38.875380
2517.202413	242995.211903	38.880397
2519.598226	243260.416558	38.885415
2521.666901	243562.554788	38.890432
2524.461912	243834.784056	38.895450
2526.746910	244127.643624	38.900468
2529.149246	244419.443840	38.905485
2531.774935	244722.487128	38.910503
2534.127491	245023.059739	38.915520
2536.648712	245323.479295	38.920538
2538.888197	245620.083265	38.925556
2541.341379	245930.090994	38.930573
2544.268634	246241.091131	38.935591
2546.874378	246554.225779	38.940608
2549.153386	246869.267162	38.945626
2551.967365	247177.975841	38.950644
2554.345066	247513.450760	38.955661
2556.899950	247820.296791	38.960679
2559.062026	248154.816705	38.965696
2561.714699	248479.734196	38.970714
2564.394665	248805.841920	38.975732
2566.933085	249137.942068	38.980749
2569.663557	249479.487193	38.985767
2572.358689	249801.606607	38.990784
2575.251219	250121.968102	38.995802
2577.784393	250466.721795	39.000820
2580.432618	250790.857344	39.005837
2583.424853	251130.916619	39.010855
2585.736448	251451.931599	39.015872
2588.143119	251796.327071	39.020890
2591.127690	252119.548231	39.025908
2593.697952	252461.683755	39.030925
2596.416726	252796.226666	39.035943
2599.061310	253134.592237	39.040960
2601.687763	253463.664205	39.045978
2604.137518	253794.466687	39.050996
2606.695042	254141.941798	39.056013
2609.599817	254464.925747	39.061031
2611.966794	254808.952172	39.066048
2614.739885	255145.497429	39.071066
2617.546484	255485.086207	39.076084
2620.128264	255826.209900	39.081101
2622.818054	256168.053709	39.086119
2625.791716	256505.915742	39.091136
2628.258663	256830.750975	39.096154
2630.646829	257174.447741	39.101172
2633.762817	257503.728169	39.106189
2636.108446	257844.562226	39.111207
2638.451028	258181.332870	39.116224
2641.381735	258517.985421	39.121242
2644.451631	258851.898319	39.126260
2646.609290	259200.435675	39.131277
2649.256765	259530.402799	39.136295
2651.703784	259844.271414	39.141312
2654.063547	260153.581746	39.146330
2656.828583	260456.248930	39.151348
2659.131149	260773.012035	39.156365
2661.955780	261088.651286	39.161383
2663.891441	261409.715500	39.166400
2666.607911	261725.677423	39.171418
2669.183569	262051.365884	39.176436
2671.463601	262390.742878	39.181453
2674.156725	262732.950737	39.186471
2676.572070	263081.172659	39.191488
2679.357262	263421.537650	39.196506
2681.830697	263776.889332	39.201524
2684.289294	264134.174358	39.206541
2687.133592	264487.740603	39.211559
2689.709842	264845.668168	39.216576
2692.240554	265220.801177	39.221594
2695.205420	265595.713352	39.226612
2697.877539	265967.395234	39.231629
2700.846459	266338.242928	39.236647
2703.420426	266714.437354	39.241664
2706.324296	267073.407263	39.246682
2709.443134	267449.312742	39.251700
2712.018330	267819.538075	39.256717
2715.234338	268195.327092	39.261735
2717.820626	268562.680605	39.266752
2720.686603	268947.061059	39.271770
2723.372409	269315.085156	39.276788
2726.097862	269685.643511	39.281805
2728.725959	270063.762271	39.286823
2731.499111	270445.998992	39.291840
2734.298642	270816.495366	39.296858
2737.411187	271200.482314	39.301876
2740.000389	271579.751071	39.306893
2742.940709	271954.798199	39.311911
2745.777081	272333.011935	39.316928
2748.570569	272713.772913	39.321946
2751.606196	273087.281074	39.326964
2753.929320	273471.215948	39.331981
2756.972549	273845.281935	39.336999
2759.843041	274226.056435	39.342016
2762.532392	274604.370135	39.347034
2765.427018	274976.910183	39.352052
2767.752117	275372.632155	39.357069
2770.819397	275752.664295	39.362087
2773.697738	276133.285224	39.367104
2776.511796	276523.849048	39.372122
2779.190543	276903.764828	39.377140
2781.721329	277290.308878	39.382157
2784.643661	277667.823452	39.387175
2787.249195	278061.366858	39.392192
2790.231892	278442.682213	39.397210
2793.220585	278824.402968	39.402228
2795.874642	279222.256935	39.407245
2798.606604	279592.230929	39.412263
2801.362329	279950.058218	39.417280
2803.881469	280296.135681	39.422298
2806.931019	280654.322609	39.427316
2809.404731	281009.348939	39.432333
2811.912789	281361.829328	39.437351
2814.633081	281721.236434	39.442368
2817.146334	282093.530189	39.447386
2819.962234	282452.134241	39.452404
2822.333589	282835.017765	39.457421
2824.947924	283212.045209	39.462439
2828.123743	283608.035883	39.467456
2830.494515	284005.804930	39.472474
2833.529403	284388.429810	39.477492
2835.967506	284808.847140	39.482509
2838.644822	285189.114657	39.487527
2841.627048	285608.657547	39.492544
2844.818685	286008.225431	39.497562
2847.607932	286426.299230	39.502580
2850.042839	286835.715432	39.507597
2852.925822	287261.495950	39.512615
2856.206361	287678.855426	39.517632
2858.659771	288113.060468	39.522650
2861.874141	288533.909536	39.527668
2864.390495	288963.657944	39.532685
2867.443800	289387.833718	39.537703
2870.310371	289820.319749	39.542720
2873.416452	290258.000164	39.547738
2876.651985	290688.038583	39.552756
2879.393570	291119.958107	39.557773
2882.465875	291564.094015	39.562791
2885.287631	291996.786855	39.567808
2888.401346	292440.990859	39.572826
2891.552700	292866.466462	39.577844
2894.449109	293301.532971	39.582861
2897.497715	293734.567769	39.587879
2900.165790	294170.278414	39.592896
2903.248039	294605.135148	39.597914
2906.437405	295035.554050	39.602932
2909.328693	295470.769461	39.607949
2912.548301	295900.673729	39.612967
2915.550785	296331.017880	39.617984
2918.387059	296756.002173	39.623002
2921.661273	297181.779859	39.628020
2924.303227	297617.792029	39.633037
2927.397345	298042.453174	39.638055
2930.264855	298486.886369	39.643072
2933.175275	298915.867422	39.648090
2936.573525	299345.887864	39.653108
2939.265878	299771.141871	39.658125
2941.953900	300197.411546	39.663143
2945.293999	300630.740102	39.668160
2948.131068	301061.810206	39.673178
2951.057825	301486.082798	39.678196
2953.939326	301922.045976	39.683213
2956.749914	302332.795790	39.688231
2959.979823	302730.777569	39.693248
2962.929587	303145.033894	39.698266
2965.512592	303516.394088	39.703284
2968.264755	303925.878702	39.708301
2971.118513	304309.284823	39.713319
2973.916110	304705.856386	39.718336
2976.429711	305130.107713	39.723354
2979.222513	305527.236499	39.728372
2981.813948	305951.472955	39.733389
2984.722610	306374.921241	39.738407
2987.869173	306801.302355	39.743424
2990.197891	307254.939014	39.748442
2993.152254	307679.595036	39.753460
2996.063986	308130.113678	39.758477
2998.996723	308582.735571	39.763495
3002.324261	309031.127727	39.768512
3004.704054	309498.006901	39.773530
3007.943856	309940.491413	39.778548
3011.165674	310422.879910	39.783565
3014.004202	310882.213529	39.788583
3017.026307	311365.467898	39.793600
3019.959254	311836.695059	39.798618
3023.335066	312324.308819	39.803636
3026.249332	312794.620516	39.808653
3029.516287	313274.500576	39.813671
3032.928981	313763.016444	39.818688
3035.733504	314238.291992	39.823706
3038.989897	314717.633852	39.828724
3042.145380	315192.722525	39.833741
3045.142510	315683.530260	39.838759
3048.556962	316160.630710	39.843776
3051.563244	316648.460705	39.848794
3055.034980	317130.525481	39.853812
3058.081976	317612.680500	39.858829
3060.805062	318107.557858	39.863847
3064.197461	318588.637415	39.868864
3067.430528	319059.326768	39.873882
3070.525242	319539.839033	39.878900
3073.598924	320031.653898	39.883917
3076.572516	320506.008760	39.888935
3079.998678	320985.470499	39.893952
3083.029878	321488.103282	39.898970
3086.445750	321958.977288	39.903988
3089.394566	322425.579867	39.909005
3092.383735	322920.160393	39.914023
3095.915790	323394.665311	39.919040
3098.693051	323879.572450	39.924058
3102.131568	324374.454359	39.929076
3105.012907	324846.692244	39.934093
3108.216062	325326.063480	39.939111
3111.576347	325813.863752	39.944128
3114.368268	326293.395947	39.949146
3117.739957	326769.811506	39.954164
3120.878502	327251.644854	39.959181
3123.575021	327717.419430	39.964199
3127.084218	328155.153791	39.969216
3129.593504	328609.499607	39.974234
3132.639480	329038.922019	39.979252
3135.582931	329493.371645	39.984269
3138.396804	329946.112233	39.989287
3141.815936	330392.380417	39.994304
3144.169469	330865.579652	39.999322
3147.306128	331321.181074	40.004340
3150.014530	331799.930135	40.009357
3152.980850	332279.930283	40.014375
3156.007100	332762.050767	40.019392
3159.104402	333263.937901	40.024410
3162.301546	333753.896430	40.029428
3165.372506	334257.050278	40.034445
3168.204914	334757.368870	40.039463
3171.794721	335259.239881	40.044480
3174.767424	335779.283999	40.049498
3177.828428	336296.110768	40.054516
3181.227671	336810.518611	40.059533
3184.322729	337337.463213	40.064551
3187.622605	337851.523204	40.069568
3191.017595	338392.224746	40.074586
3194.480953	338902.873552	40.079604
3197.641919	339424.560304	40.084621
3200.565213	339962.073254	40.089639
3204.245532	340476.889941	40.094656
3207.618863	341030.394599	40.099674
3210.813493	341549.265513	40.104692
3214.274092	342068.064598	40.109709
3217.687499	342614.591950	40.114727
3220.879385	343132.992860	40.119744
3224.177339	343667.748390	40.124762
3227.257026	344212.714531	40.129780
3230.877108	344737.787174	40.134797
3234.041639	345268.030231	40.139815
3237.733696	345797.296444	40.144832
3240.899437	346334.130472	40.149850
3244.201194	346848.241512	40.154868
3247.893074	347387.013452	40.159885
3251.307660	347916.837111	40.164903
3254.479787	348431.969771	40.169920
3257.741292	348958.659828	40.174938
3260.729042	349485.413572	40.179956
3264.104475	350014.842652	40.184973
3267.439074	350541.632934	40.189991
3270.693417	351069.649306	40.195008
3274.171643	351599.402068	40.200026
3277.436013	352138.855139	40.205044
3280.681664	352659.723983	40.210061
3283.954040	353198.606525	40.215079
3286.880841	353719.489922	40.220096
3290.270682	354253.900739	40.225114
3293.486054	354774.702516	40.230132
3296.974745	355314.671139	40.235149
3300.006135	355837.014221	40.240167
3303.397672	356331.728976	40.245184
3306.624603	356831.135341	40.250202
3309.726171	357320.961949	40.255220
3312.995362	357801.162717	40.260237
3315.817151	358296.354228	40.265255
3319.154534	358796.535567	40.270272
3322.327678	359312.753503	40.275290
3325.635167	359808.258985	40.280308
3328.770702	360312.010019	40.285325
3331.517161	360844.649797	40.290343
3335.061481	361368.502719	40.295360
3338.166981	361895.515630	40.300378
3341.585940	362430.620010	40.305396
3344.580056	362962.739913	40.310413
3347.528701	363526.813427	40.315431
3350.976408	364068.366138	40.320448
3354.200168	364638.498871	40.325466
3357.716088	365182.489352	40.330484
3361.297067	365756.180700	40.335501
3364.529830	366329.412262	40.340519
3368.223321	366889.951075	40.345536
3371.438154	367462.358859	40.350554
3374.688344	368046.020912	40.355572
3378.317575	368610.786001	40.360589
3381.614132	369201.733736	40.365607
3385.066534	369782.828389	40.370624
3388.946135	370362.578898	40.375642
3392.381805	370947.974273	40.380660
3395.892570	371522.134130	40.385677
3398.924550	372109.455069	40.390695
3402.859515	372700.837114	40.395712
3406.223627	373282.151623	40.400730
3409.428218	373877.235539	40.405748
3413.023624	374457.710432	40.410765
3416.506968	375056.082481	40.415783
3419.585107	375655.296373	40.420800
3423.339952	376244.727783	40.425818
3426.689900	376835.153350	40.430836
3430.440590	377432.458534	40.435853
3433.754792	378044.031351	40.440871
3437.318855	378629.702945	40.445888
3441.253033	379239.814625	40.450906
3444.359934	379841.016075	40.455924
3448.719117	380420.268946	40.460941
3451.896432	381017.508858	40.465959
3455.002536	381600.214726	40.470976
3458.850366	382198.700163	40.475994
3462.139819	382803.048277	40.481012
3465.845435	383386.037940	40.486029
3468.698406	383979.452283	40.491047
3472.787929	384573.803222	40.496064
3476.204732	385148.567075	40.501082
3479.701505	385768.257095	40.506100
3483.303717	386352.180606	40.511117
3487.234386	386925.880598	40.516122
3490.388624	387466.290730	40.521127
3493.194590	387947.091795	40.526132
3495.790186	388405.746036	40.531136
3498.566161	388773.968472	40.536141
3500.878289	389118.332677	40.541146
3503.627099	389397.402174	40.546151
3505.526328	389645.149782	40.551156
3507.115642	389849.412768	40.556160
3509.401715	389995.844246	40.561165
3510.571602	390122.745397	40.566170
3511.789673	390193.673088	40.571175
3513.117524	390236.333627	40.576180
3513.821897	390269.303196	40.581184
3514.992338	390266.194130	40.586189
3515.493944	390237.000743	40.591194
3515.982255	390186.348816	40.596199
3516.369438	390118.091669	40.601204
3516.668510	390037.719459	40.606208
3516.858052	389932.928600	40.611213
3517.346742	389829.386948	40.616218
3517.714598	389710.988943	40.621223
3517.836324	389580.983562	40.626228
3517.467281	389444.418632	40.631232
3517.630480	389300.115241	40.636237
3517.414725	389160.753352	40.641242
3517.393628	388995.626892	40.646247
3517.404689	388851.116889	40.651252
3517.207859	388712.080831	40.656256
3517.190118	388536.195543	40.661261
3516.513184	388383.273885	40.666266
3516.375806	388223.502258	40.671271
3516.277538	388073.183249	40.676276
3515.746914	387924.889986	40.681280
3516.010716	387761.162277	40.686285
3515.192964	387612.963984	40.691290
3515.160482	387470.133657	40.696295
3515.111468	387319.574873	40.701300
3514.415813	387193.148476	40.706304
3514.256691	387039.223829	40.711309
3513.964939	386903.450807	40.716314
3514.061112	386772.447597	40.721319
3513.976388	386636.284840	40.726324
3513.238375	386514.796167	40.731328
3513.359764	386368.911052	40.736333
3512.865076	386253.181079	40.741338
3512.969443	386118.588601	40.746343
3512.756046	386007.823126	40.751348
3512.287074	385886.544146	40.756352
3512.208929	385756.175195	40.761357
3511.888251	385666.761747	40.766362
3511.593652	385539.096445	40.771367
3511.628369	385434.393356	40.776372
3511.006399	385326.208054	40.781376
3511.207083	385223.436295	40.786381
3510.955926	385133.959708	40.791386
3510.575185	385036.594386	40.796391
3510.665236	384941.341446	40.801396
3510.470891	384841.428482	40.806400
3510.020550	384750.558323	40.811405
3509.963994	384670.688237	40.816410
3509.881454	384579.759517	40.821415
3509.692059	384502.605778	40.826420
3509.460724	384422.813654	40.831424
3509.420277	384334.293656	40.836429
3509.154642	384269.282247	40.841434
3508.821919	384201.916204	40.846439
3508.772802	384134.098303	40.851444
3508.422905	384072.583988	40.856448
3508.387374	383998.049765	40.861453
3507.948395	383944.814589	40.866458
3507.845157	383889.033960	40.871463
3508.396493	383832.971747	40.876468
3508.086190	383783.327303	40.881472
3508.227767	383711.485709	40.886477
3508.192184	383657.830312	40.891482
3507.899323	383605.080192	40.896487
3507.857416	383542.727933	40.901492
3507.672594	383487.646266	40.906496
3507.817704	383447.008586	40.911501
3507.640721	383392.027268	40.916506
3507.485825	383336.355714	40.921511
3507.699602	383286.856654	40.926516
3507.448937	383238.880581	40.931520
3507.686667	383182.714386	40.936525
3507.275128	383139.595726	40.941530
3507.065517	383106.948594	40.946535
3507.220802	383053.414756	40.951540
3506.877684	383015.676771	40.956544
3506.927986	382962.998666	40.961549
3506.627250	382929.119603	40.966554
3506.674255	382877.026843	40.971559
3507.047540	382834.190683	40.976564
3506.866563	382817.408575	40.981568
3506.915622	382760.940960	40.986573
3506.612605	382727.367266	40.991578
3506.580368	382676.838138	40.996583
3506.417774	382646.700992	41.001588
3506.236039	382622.874113	41.006592
3506.435269	382582.176084	41.011597
3505.795183	382563.889624	41.016602
3506.017009	382526.773954	41.021607
3506.055607	382492.459368	41.026612
3505.730583	382480.888135	41.031616
3506.072910	382447.135876	41.036621
3506.234022	382419.439774	41.041626
3505.888383	382392.459580	41.046631
3506.007887	382371.077324	41.051636
3505.989133	382340.459407	41.056640
3505.950354	382310.556748	41.061645
3505.817554	382285.704613	41.066650
3505.844241	382244.855471	41.071655
3506.006557	382224.788869	41.076660
3505.610271	382213.406848	41.081664
3505.678527	382170.084074	41.086669
3505.553561	382145.968161	41.091674
3505.320720	382139.697713	41.096679
3505.754532	382107.889021	41.101684
3505.572220	382095.023466	41.106688
3505.402510	382069.998995	41.111693
3505.299707	382063.987739	41.116698
3505.406044	382037.342768	41.121703
3505.338822	382019.652173	41.126708
3505.221018	382006.115134	41.131712
3505.291956	381982.680271	41.136717
3505.250756	381965.901123	41.141722
3505.343423	381949.253403	41.146727
3505.336813	381916.624022	41.151732
3505.580602	381906.107177	41.156736
3505.606690	381876.880615	41.161741
3505.288546	381864.341651	41.166746
3505.129422	381847.860857	41.171751
3505.267917	381837.411504	41.176756
3505.130806	381812.788640	41.181760
3505.086514	381801.325418	41.186765
3505.423666	381781.714173	41.191770
3505.321351	381766.139954	41.196775
3505.387302	381753.413069	41.201780
3505.250949	381735.835003	41.206784
3505.264044	381697.301838	41.211789
3505.353097	381695.583828	41.216794
3505.179532	381669.466079	41.221799
3505.683962	381647.895402	41.226804
3505.152695	381636.814313	41.231808
3505.329555	381625.595842	41.236813
3505.199831	381609.949593	41.241818
3504.879632	381581.616844	41.246823
3505.023639	381573.531837	41.251828
3504.747126	381559.689098	41.256832
3505.157190	381536.124051	41.261837
3504.986301	381522.340900	41.266842
3504.452638	381526.240341	41.271847
3505.215760	381507.909579	41.276852
3504.532629	381504.431570	41.281856
3504.738729	381498.702025	41.286861
3504.926073	381472.857720	41.291866
3504.836130	381461.859413	41.296871
3504.821529	381450.162493	41.301876
3504.861786	381442.958592	41.306880
3505.337715	381422.969159	41.311885
3505.085659	381418.710863	41.316890
3504.637457	381404.055909	41.321895
3505.178711	381391.609832	41.326900
3505.234460	381376.061333	41.331904
3505.153455	381359.084746	41.336909
3504.858297	381328.738616	41.341914
3505.120424	381321.321584	41.346919
3505.232851	381315.072719	41.351924
3504.807991	381307.281054	41.356928
3505.499815	381284.154544	41.361933
3505.289556	381263.841138	41.366938
3504.897883	381246.735579	41.371943
3505.120334	381225.056641	41.376948
3504.967649	381214.576851	41.381952
3505.234545	381202.453853	41.386957
3504.985833	381195.651656	41.391962
3504.866468	381178.808221	41.396967
3505.084878	381153.798096	41.401972
3504.686608	381155.514322	41.406976
3504.677966	381134.787472	41.411981
3504.941907	381112.644109	41.416986
3504.525448	381123.010610	41.421991
3504.876739	381098.360945	41.426996
3504.622787	381096.976901	41.432000
3504.820579	381071.690213	41.437005
3504.668935	381074.130462	41.442010
3504.839907	381059.224893	41.447015
3505.008288	381040.682727	41.452020
3504.695691	381024.785380	41.457024
3504.902894	381006.669431	41.462029
3504.536019	381001.157560	41.467034
3504.607830	380982.071093	41.472039
3504.766257	380975.458830	41.477044
3504.859183	380977.326316	41.482048
3504.606222	380959.944365	41.487053
3504.793022	380956.354215	41.492058
3504.887533	380934.390136	41.497063
3505.149647	380923.208851	41.502068
3504.743859	380915.515825	41.507072
3504.978470	380897.471793	41.512077
3504.771058	380882.931178	41.517082
3504.442824	380880.643257	41.522087
3504.590428	380863.325107	41.527092
3504.673260	380846.449562	41.532096
3504.804973	380846.276226	41.537101
3504.716375	380830.089050	41.542106
3504.520181	380826.915506	41.547111
3505.100618	380815.607567	41.552116
3504.692433	380810.916078	41.557120
3504.467358	380800.447618	41.562125
3504.580508	380775.453889	41.567130
3504.776388	380770.081924	41.572135
3504.786294	380762.221417	41.577140
3504.745609	380751.596626	41.582144
3504.827026	380734.975593	41.587149
3504.050803	380737.667203	41.592154
3504.532935	380726.552814	41.597159
3504.583495	380707.520439	41.602164
3503.951772	380727.636782	41.607168
3504.452953	380697.113397	41.612173
3504.577140	380703.299699	41.617178
3504.529427	380705.214865	41.622183
3504.868302	380683.618953	41.627188
3504.893329	380685.624356	41.632192
3504.934088	380660.641996	41.637197
3504.818928	380650.664796	41.642202
3504.563647	380651.926065	41.647207
3504.680068	380619.454171	41.652212
3504.573920	380610.950700	41.657216
3504.444450	380594.922490	41.662221
3504.660412	380613.327986	41.667226
3504.760933	380587.929190	41.672231
3504.556913	380573.922032	41.677236
3504.306697	380585.788428	41.682240
3504.843856	380549.918126	41.687245
3504.543753	380537.782819	41.692250
3504.696927	380541.650080	41.697255
3504.566868	380520.840359	41.702260
3504.262140	380534.622932	41.707264
3504.690079	380516.115784	41.712269
3504.893541	380491.692574	41.717274
3504.109480	380497.437510	41.722279
3504.621423	380476.449972	41.727284
3504.322793	380465.865880	41.732288
3504.578635	380454.100471	41.737293
3504.156533	380467.977924	41.742298
3504.309043	380442.596248	41.747303
3504.450123	380442.726638	41.752308
3504.564804	380434.951236	41.757312
3504.644903	380430.411415	41.762317
3504.735160	380427.497762	41.767322
3504.337481	380425.169924	41.772327
3504.442732	380402.059317	41.777332
3504.386477	380390.444963	41.782336
3504.701660	380390.878471	41.787341
3504.690137	380382.080216	41.792346
3504.438258	380385.121336	41.797351
3504.859266	380365.140039	41.802356
3504.292698	380355.869975	41.807360
3504.410156	380345.779622	41.812365
3504.754524	380341.070842	41.817370
3504.471286	380319.140698	41.822375
3504.857582	380313.306189	41.827380
3504.563096	380308.418626	41.832384
3504.547505	380289.396503	41.837389
3504.295742	380295.413396	41.842394
3504.231403	380285.962184	41.847399
3504.211922	380263.379893	41.852404
3504.039403	380261.525133	41.857408
3504.050586	380277.572356	41.862413
3504.514216	380279.991690	41.867418
3504.368736	380249.773654	41.872423
3504.774302	380246.886444	41.877428
3504.579541	380243.432851	41.882432
3504.667428	380221.418547	41.887437
3504.470759	380222.746865	41.892442
3504.469110	380216.007175	41.897447
3504.420495	380189.665198	41.902452
3504.250778	380192.388134	41.907456
3504.459704	380195.610763	41.912461
3504.618180	380174.424599	41.917466
3504.454991	380159.062828	41.922471
3504.152475	380164.451911	41.927476
3504.329662	380159.667802	41.932480
3504.515390	380142.572211	41.937485
3504.888257	380139.435821	41.942490
3504.331084	380122.864610	41.947495
3504.346123	380111.009994	41.952500
3504.324106	380121.263537	41.957504
3504.356649	380101.165477	41.962509
3504.388332	380091.826209	41.967514
3504.133577	380082.837430	41.972519
3504.374253	380086.487430	41.977524
3504.472300	380077.442877	41.982528
3504.555362	380069.672401	41.987533
3504.748043	380059.061397	41.992538
3504.889689	380053.290960	41.997543
3504.700713	380036.661506	42.002548
3504.360562	380034.782366	42.007552
3504.238897	380018.905290	42.012557
3504.300542	380019.633226	42.017562
3504.111304	380010.964719	42.022567
3504.449431	380006.256886	42.027572
3504.198346	379992.969118	42.032576
3504.334940	379977.203804	42.037581
3504.385638	379971.829246	42.042586
3504.264630	379983.319319	42.047591
3504.367404	379968.373244	42.052596
3504.266061	379972.128192	42.057600
3504.500048	379952.506895	42.062605
3504.655042	379958.027155	42.067610
3504.272181	379934.510182	42.072615
3504.511199	379931.216895	42.077620
3504.255559	379928.612229	42.082624
3503.860868	379913.566735	42.087629
3503.895064	379909.873442	42.092634
3503.928223	379907.121383	42.097639
3504.169884	379904.234624	42.102644
3504.022372	379920.586860	42.107648
3504.420189	379910.528375	42.112653
3504.428515	379896.868919	42.117658
3504.435540	379895.265535	42.122663
3504.597366	379884.761098	42.127668
3504.191174	379887.139924	42.132672
3504.434569	379860.827865	42.137677
3504.375472	379854.148063	42.142682
3504.310859	379863.391033	42.147687
3504.276957	379836.817583	42.152692
3504.296288	379842.410174	42.157696
3504.235912	379838.299441	42.162701
3504.041990	379836.727821	42.167706
3504.149303	379831.293426	42.172711
3504.244336	379811.058166	42.177716
3504.180063	379810.330818	42.182720
3504.218966	379812.741022	42.187725
3504.431677	379808.968630	42.192730
3504.112082	379798.006154	42.197735
3504.671985	379785.658354	42.202740
3504.327303	379801.990940	42.207744
3504.453556	379767.227686	42.212749
3504.306674	379763.715612	42.217754
3504.482857	379774.319430	42.222759
3504.518521	379746.971889	42.227764
3504.179818	379742.269285	42.232768
3504.463358	379735.179214	42.237773
3504.442479	379724.169495	42.242778
3504.054574	379718.380985	42.247783
3504.237640	379709.729858	42.252788
3504.288819	379701.735439	42.257792
3504.253614	379710.541411	42.262797
3504.697206	379692.896170	42.267802
3504.256267	379672.287748	42.272807
3504.172380	379679.219272	42.277812
3504.249503	379691.161364	42.282816
3504.597315	379669.258265	42.287821
3504.472954	379656.204693	42.292826
3504.472395	379650.965367	42.297831
3504.718885	379627.526759	42.302836
3504.279649	379628.918878	42.307840
3504.249391	379613.841091	42.312845
3504.578431	379623.530577	42.317850
3504.448882	379592.495609	42.322855
3504.498366	379598.414117	42.327860
3504.195489	379597.419271	42.332864
3504.222065	379567.453286	42.337869
3504.296118	379560.726949	42.342874
3504.227603	379556.973557	42.347879
3504.423362	379560.605272	42.352884
3504.331700	379556.626628	42.357888
3504.206177	379540.292146	42.362893
3504.199027	379543.777898	42.367898
3504.155982	379549.965386	42.372903
3504.229377	379530.369266	42.377908
3504.314136	379525.701430	42.382912
3504.220589	379513.863799	42.387917
3504.483173	379510.159797	42.392922
3504.218863	379501.782825	42.397927
3504.468504	379477.351680	42.402932
3504.726495	379488.171554	42.407936
3504.463628	379471.935058	42.412941
3504.518396	379459.132884	42.417946
3504.136080	379448.027617	42.422951
3504.505783	379447.791218	42.427956
3504.229800	379440.713243	42.432960
3504.214859	379424.488404	42.437965
3504.153083	379423.760654	42.442970
3504.315010	379424.447313	42.447975
3504.345440	379398.728173	42.452980
3504.247985	379403.525380	42.457984
3504.414624	379389.510070	42.462989
3504.498769	379390.183591	42.467994
3504.252270	379372.469257	42.472999
3504.531625	379372.348879	42.478004
3504.275290	379372.058840	42.483008
3504.215733	379355.993634	42.488013
3504.305422	379333.139200	42.493018
3504.264308	379336.401428	42.498023
3504.460479	379334.997031	42.503028
3504.086668	379321.092568	42.508032
3504.192522	379305.891406	42.513037
3504.198624	379311.358991	42.518042
3504.298390	379312.945694	42.523047
3504.437293	379303.767330	42.528052
3504.254709	379286.907633	42.533056
3504.192555	379296.837086	42.538061
3504.541440	379287.803566	42.543066
3504.258171	379271.595648	42.548071
3504.458217	379250.453281	42.553076
3504.017394	379256.144136	42.558080
3504.216182	379253.925411	42.563085
3504.350973	379247.825287	42.568090
3503.820285	379227.688644	42.573095
3504.322257	379226.846334	42.578100
3504.131553	379224.180486	42.583104
3504.368631	379228.238091	42.588109
3504.331773	379214.967062	42.593114
3504.178438	379207.996829	42.598119
3504.208266	379197.055250	42.603124
3504.288990	379213.626047	42.608128
3504.306740	379196.403990	42.613133
3504.202190	379179.175823	42.618138
3504.039315	379170.274049	42.623143
3504.420040	379171.612863	42.628148
3504.204652	379178.616134	42.633152
3503.967422	379158.204150	42.638157
3504.004330	379151.661659	42.643162
3504.035949	379147.460006	42.648167
3504.534421	379141.836504	42.653172
3503.900084	379151.424056	42.658176
3504.049275	379132.960321	42.663181
3504.208470	379128.331540	42.668186
3503.904131	379127.031695	42.673191
3504.365315	379111.723415	42.678196
3504.235448	379112.685122	42.683200
3503.870103	379131.335824	42.688205
3504.024073	379129.582004	42.693210
3503.837003	379114.477945	42.698215
3504.394092	379107.649734	42.703220
3503.999431	379116.512665	42.708224
3504.294394	379113.541118	42.713229
3504.210416	379116.199704	42.718234
3503.832374	379103.033443	42.723239
3504.034183	379090.563990	42.728244
3503.928813	379091.598130	42.733248
3503.994437	379086.297396	42.738253
3503.999527	379088.255163	42.743258
3503.928228	379102.586339	42.748263
3504.336887	379093.746803	42.753268
3504.221572	379082.115962	42.758272
3503.851394	379070.271058	42.763277
3504.101236	379082.720163	42.768282
3504.037087	379083.696917	42.773287
3503.950777	379077.911504	42.778292
3504.054821	379079.319496	42.783296
3504.171419	379056.664126	42.788301
3504.164126	379050.281215	42.793306
3503.867393	379043.130144	42.798311
3504.446872	379035.153812	42.803316
3503.797569	379051.662042	42.808321
3504.080773	379047.598649	42.813325
3504.152105	379033.649148	42.818330
3503.898556	379020.946441	42.823335
3504.414582	379018.346898	42.828340
3504.113422	379034.291400	42.833345
3504.071113	379025.497707	42.838349
3503.857786	379004.166208	42.843354
3503.897419	378995.384989	42.848359
3504.062132	378980.505050	42.853364
3504.162595	378991.121050	42.858369
3504.086275	378996.042141	42.863373
3504.290358	378999.036720	42.868378
3504.250797	378984.189076	42.873383
3504.424963	378966.331752	42.878388
3504.192203	378970.031266	42.883393
3504.120082	378965.439034	42.888397
3504.334235	378965.150918	42.893402
3504.142937	378958.975126	42.898407
3504.483474	378934.224054	42.903412
3504.224808	378939.987897	42.908417
3504.033538	378931.879040	42.913421
3504.168445	378908.584817	42.918426
3504.035930	378918.601794	42.923431
3504.106250	378909.968314	42.928436
3504.136616	378915.228639	42.933441
3504.294353	378909.658970	42.938445
3504.260758	378904.679116	42.943450
3503.856616	378901.436548	42.948455
3504.483208	378878.802193	42.953460
3504.264347	378884.763230	42.958465
3503.839486	378881.396762	42.963469
3504.079601	378869.506188	42.968474
3503.983128	378865.884324	42.973479
3504.290906	378859.883969	42.978484
3504.241963	378852.948040	42.983489
3504.315081	378864.026227	42.988493
3504.440914	378844.396040	42.993498
3504.029994	378833.142510	42.998503
3504.019668	378827.573963	43.003508
3503.990800	378831.190387	43.008513
3504.105392	378833.003681	43.013517
3504.283764	378830.203154	43.018522
3504.114004	378809.042708	43.023527
3504.096007	378817.617244	43.028532
3504.196146	378812.336452	43.033537
3504.136089	378802.070283	43.038541
3504.168831	378787.974185	43.043546
3503.949641	378776.156194	43.048551
3504.461758	378767.503711	43.053556
3504.124421	378780.274653	43.058561
3504.212888	378778.810958	43.063565
3504.554584	378766.802555	43.068570
3504.066653	378757.519678	43.073575
3504.098383	378745.585705	43.078580
3504.170374	378755.850178	43.083585
3504.093100	378750.241334	43.088589
3504.368246	378723.720013	43.093594
3504.034403	378728.045972	43.098599
3504.633659	378715.945966	43.103604
3504.375104	378708.305531	43.108609
3504.183487	378702.613016	43.113613
3504.176701	378689.159009	43.118618
3504.067811	378697.417284	43.123623
3504.222603	378688.744967	43.128628
3504.182677	378679.492988	43.133633
3504.039382	378657.310872	43.138637
3504.029234	378658.406275	43.143642
3504.038526	378664.712804	43.148647
3504.124857	378661.443549	43.153652
3504.361064	378666.188099	43.158657
3504.330436	378654.823529	43.163661
3504.216621	378637.138758	43.168666
3504.269398	378631.763689	43.173671
3504.335839	378629.006278	43.178676
3504.269693	378618.512108	43.183681
3503.938799	378610.806785	43.188685
3504.462686	378601.338480	43.193690
3504.002943	378604.183680	43.198695
3504.283098	378597.806125	43.203700
3504.067195	378581.638142	43.208705
3504.141903	378579.591606	43.213709
3504.329692	378565.674399	43.218714
3504.259207	378583.185033	43.223719
3504.407623	378557.701043	43.228724
3504.093002	378547.398745	43.233729
3504.200913	378544.838254	43.238733
3504.321292	378541.665348	43.243738
3503.789615	378543.199294	43.248743
3504.030818	378521.465021	43.253748
3504.156977	378514.577657	43.258753
3504.044260	378519.809783	43.263757
3504.266083	378525.548597	43.268762
3504.301092	378519.362395	43.273767
3504.228838	378506.147592	43.278772
3503.999402	378493.466338	43.283777
3504.212688	378490.711139	43.288781
3504.255019	378487.296214	43.293786
3504.292094	378483.653203	43.298791
3504.271095	378458.958988	43.303796
3504.342684	378461.008014	43.308801
3504.127399	378470.376873	43.313805
3504.364940	378471.840088	43.318810
3504.277017	378445.808377	43.323815
3503.887152	378434.169876	43.328820
3503.769244	378436.554084	43.333825
3503.943447	378423.681821	43.338829
3504.079400	378420.862537	43.343834
3503.872820	378438.471055	43.348839
3504.221164	378427.733262	43.353844
3504.409775	378412.569543	43.358849
3504.333688	378414.616482	43.363853
3504.378821	378398.763252	43.368858
3504.177802	378395.971802	43.373863
3504.386017	378375.056593	43.378868
3504.009697	378369.367793	43.383873
3503.982081	378372.348178	43.388877
3504.223893	378360.406313	43.393882
3504.181517	378366.212352	43.398887
3504.382753	378346.417385	43.403892
3504.300969	378340.707453	43.408897
3504.115112	378337.633813	43.413901
3504.351132	378334.468044	43.418906
3504.068011	378321.820657	43.423911
3504.086714	378309.456211	43.428916
3503.870578	378310.660494	43.433921
3503.873957	378312.058992	43.438925
3504.129465	378305.837898	43.443930
3504.143145	378313.059463	43.448935
3504.013920	378295.402410	43.453940
3504.496236	378274.545558	43.458945
3504.341552	378282.226146	43.463949
3504.222654	378277.285133	43.468954
3504.041785	378269.174496	43.473959
3504.184520	378250.406144	43.478964
3504.193293	378254.347330	43.483969
3503.542790	378237.383108	43.488973
3504.038430	378242.976935	43.493978
3504.052882	378249.028361	43.498983
3504.120667	378249.907972	43.503988
3504.212627	378248.825237	43.508993
3504.095599	378228.444639	43.513997
3504.171116	378224.541173	43.519002
3503.999468	378227.671516	43.524007
3504.019316	378227.439548	43.529012
3504.246476	378228.243093	43.534017
3503.906156	378210.237843	43.539021
3503.953758	378196.317233	43.544026
3503.992595	378195.675296	43.549031
3503.822828	378195.956577	43.554036
3504.311099	378192.547435	43.559041
3504.125643	378197.689361	43.564045
3504.263150	378188.103992	43.569050
3503.711771	378175.371790	43.574055
3503.945402	378176.454103	43.579060
3504.020659	378171.685868	43.584065
3504.262865	378169.231300	43.589069
3504.270873	378167.398770	43.594074
3504.159424	378160.625214	43.599079
3503.817452	378140.712535	43.604084
3503.939984	378144.991845	43.609089
3503.830270	378131.808275	43.614093
3504.044087	378143.373130	43.619098
3503.594116	378140.239486	43.624103
3504.163974	378146.203125	43.629108
3504.053888	378151.231401	43.634113
3504.151924	378149.766170	43.639117
3504.281702	378118.485561	43.644122
3503.924541	378117.804483	43.649127
3503.962496	378105.894768	43.654132
3503.712789	378125.188985	43.659137
3503.785806	378116.249681	43.664141
3504.157426	378126.339773	43.669146
3503.879544	378142.942276	43.674151
3503.989322	378116.751917	43.679156
3504.014521	378097.696849	43.684161
3503.839200	378100.090153	43.689165
3503.824184	378094.064405	43.694170
3503.994505	378099.048358	43.699175
3503.903885	378099.164514	43.704180
3503.866673	378104.079534	43.709185
3504.035334	378108.427861	43.714189
3504.104672	378096.869279	43.719194
3503.896751	378076.172312	43.724199
3504.234889	378074.592815	43.729204
3504.011709	378079.537236	43.734209
3503.969541	378078.094167	43.739213
3504.027787	378085.232422	43.744218
3503.889373	378085.279827	43.749223
3504.016668	378065.954248	43.754228
3503.799122	378057.951107	43.759233
3503.999626	378049.347730	43.764237
3504.356021	378039.015528	43.769242
3504.034232	378059.745561	43.774247
3504.037698	378043.364630	43.779252
3504.217339	378051.246765	43.784257
3503.929204	378031.071165	43.789261
3504.049343	378023.218118	43.794266
3504.155509	378020.149159	43.799271
3504.443583	378005.554578	43.804276
3503.980836	378018.625381	43.809281
3504.207965	378013.171794	43.814285
3504.394414	377989.309300	43.819290
3503.911073	377983.789976	43.824295
3503.872766	377976.496115	43.829300
3504.197879	377982.676519	43.834305
3504.193824	377983.364008	43.839309
3504.110503	377956.034035	43.844314
3503.648160	377948.323927	43.849319
3503.856892	377949.944330	43.854324
3504.095643	377952.094134	43.859329
3504.279728	377957.025059	43.864333
3504.430146	377944.894032	43.869338
3503.868343	377944.804886	43.874343
3503.903202	377924.349250	43.879348
3504.071997	377922.821953	43.884353
3503.868689	377927.279975	43.889357
3503.823001	377921.716891	43.894362
3503.994033	377927.514693	43.899367
3503.843853	377927.742007	43.904372
3503.905890	377929.767136	43.909377
3503.883676	377930.864466	43.914381
3503.865201	377907.390418	43.919386
3504.012233	377902.280140	43.924391
3503.825934	377892.313484	43.929396
3503.989904	377890.532593	43.934401
3503.936078	377893.517158	43.939405
3504.116108	377900.178352	43.944410
3503.814848	377904.931654	43.949415
3504.321837	377902.155419	43.954420
3503.920274	377890.594914	43.959425
3504.163639	377877.558927	43.964429
3504.211580	377868.165689	43.969434
3503.769509	377874.492828	43.974439
3503.717775	377866.743228	43.979444
3504.048292	377873.558686	43.984449
3503.980999	377883.082336	43.989453
3504.389481	377866.942532	43.994458
3503.896126	377855.167607	43.999463
3503.958071	377847.247418	44.004468
3504.038663	377852.042103	44.009473
3503.630969	377856.074602	44.014477
3503.951573	377853.327829	44.019482
3504.110296	377858.237339	44.024487
3504.119257	377844.246408	44.029492
3504.142782	377818.272973	44.034497
3503.745394	377818.666547	44.039501
3504.113214	377823.797363	44.044506
3503.882401	377827.700160	44.049511
3504.170579	377823.661292	44.054516
3503.958447	377823.211638	44.059521
3503.638401	377824.915640	44.064525
3504.136736	377801.843105	44.069530
3503.952753	377802.864270	44.074535
3503.734681	377799.439581	44.079540
3503.913996	377794.578543	44.084545
3504.263272	377800.704285	44.089549
3504.276274	377801.389081	44.094554
3504.004926	377810.614343	44.099559
3504.331732	377774.520410	44.104564
3504.272404	377770.714523	44.109569
3504.058770	377773.800667	44.114573
3504.377237	377766.730158	44.119578
3504.020822	377757.985840	44.124583
3504.094433	377750.038351	44.129588
3504.126389	377736.501589	44.134593
3503.866792	377736.746202	44.139597
3504.117891	377741.615688	44.144602
3504.011494	377744.837496	44.149607
3504.206658	377727.306958	44.154612
3504.254889	377711.173171	44.159617
3503.917463	377705.172898	44.164621
3504.257511	377712.673642	44.169626
3504.129222	377708.726037	44.174631
3503.931920	377702.194896	44.179636
3504.020090	377691.726956	44.184641
3504.028608	377676.515120	44.189645
3503.949098	377674.925326	44.194650
3503.888979	377675.469069	44.199655
3504.239549	377676.482038	44.204660
3504.119137	377668.794128	44.209665
3503.834658	377675.223564	44.214669
3504.070164	377671.574544	44.219674
3503.717785	377652.935053	44.224679
3503.827383	377649.077014	44.229684
3503.722405	377645.736176	44.234689
3503.962362	377643.536289	44.239693
3503.998918	377648.872111	44.244698
3503.669302	377659.403844	44.249703
3504.077732	377657.838655	44.254708
3504.077514	377648.300364	44.259713
3503.627900	377655.340932	44.264717
3503.951226	377656.663437	44.269722
3503.796421	377636.797224	44.274727
3503.819781	377630.612725	44.279732
3503.735983	377622.283123	44.284737
3503.635724	377634.482801	44.289741
3503.912763	377628.410813	44.294746
3503.555101	377639.837237	44.299751
3503.990395	377625.931446	44.304756
3504.061325	377629.608510	44.309761
3503.617155	377627.771132	44.314765
3503.826393	377636.818716	44.319770
3503.591459	377640.035417	44.324775
3503.799748	377634.762807	44.329780
3503.818573	377638.600722	44.334785
3503.908622	377639.782056	44.339789
3504.117912	377639.927109	44.344794
3503.898071	377631.619016	44.349799
3503.946647	377616.222773	44.354804
3504.049859	377608.804729	44.359809
3503.781408	377614.900975	44.364813
3503.926153	377613.886185	44.369818
3504.042113	377609.213191	44.374823
3503.764838	377610.401724	44.379828
3503.889856	377607.762161	44.384833
3504.021907	377608.962292	44.389837
3504.002483	377597.010625	44.394842
3503.778234	377599.793231	44.399847
3503.834272	377583.174878	44.404852
3504.026681	377572.970222	44.409857
3503.874032	377591.435407	44.414861
3503.919727	377584.814961	44.419866
3503.852885	377596.805882	44.424871
3504.022196	377589.453692	44.429876
3504.050987	377590.797327	44.434881
3503.968970	377585.443425	44.439885
3504.127788	377556.803107	44.444890
3503.794618	377554.439462	44.449895
3504.060220	377554.982586	44.454900
3504.305571	377555.325425	44.459905
3503.940947	377559.020479	44.464909
3503.780292	377560.622986	44.469914
3504.261317	377558.105191	44.474919
3504.145969	377529.508196	44.479924
3503.879792	377530.898464	44.484929
3503.703178	377535.250566	44.489933
3504.360376	377522.962988	44.494938
3504.084662	377527.457937	44.499943
3503.966908	377517.632966	44.504948
3503.923785	377494.315186	44.509953
3503.810471	377496.673288	44.514957
3504.375635	377488.317372	44.519962
3503.988629	377486.216592	44.524967
3504.047055	377482.366627	44.529972
3504.431720	377484.035544	44.534977
3504.050560	377472.446256	44.539981
3504.191934	377464.564306	44.544986
3503.526692	377475.606991	44.549991
3504.170410	377471.766241	44.554996
3504.165851	377461.872490	44.560001
3503.919169	377479.106234	44.565005
3504.169662	377456.530526	44.570010
3504.120243	377442.752170	44.575015
3504.081627	377425.843484	44.580020
3504.096809	377435.201588	44.585025
3503.856902	377437.757757	44.590029
3504.279985	377434.791268	44.595034
3504.006016	377425.296200	44.600039
3503.597722	377412.592004	44.605044
3503.646311	377414.822772	44.610049
3503.688848	377410.466593	44.615053
3504.074146	377406.132535	44.620058
3503.870615	377420.383480	44.625063
3503.704891	377415.169968	44.630068
3504.430934	377405.720294	44.635073
3503.947877	377423.093173	44.640077
3504.157049	377412.071877	44.645082
3504.020392	377390.549337	44.650087
3503.812075	377383.689219	44.655092
3504.060015	377385.150831	44.660097
3503.909988	377381.995144	44.665101
3503.734685	377384.363052	44.670106
3504.016198	377392.941420	44.675111
3504.308349	377369.646872	44.680116
3504.032632	377380.449953	44.685121
3503.604792	377372.149251	44.690125
3503.936605	377356.199413	44.695130
3503.783877	377359.657500	44.700135
3503.670227	377368.196599	44.705140
3504.133791	377366.292015	44.710145
3503.867604	377380.934418	44.715149
3504.264330	377363.066625	44.720154
3503.870331	377381.646370	44.725159
3504.058809	377369.203921	44.730164
3503.998738	377338.792098	44.735169
3503.940258	377355.131320	44.740173
3503.959356	377332.083404	44.745178
3503.773672	377333.791621	44.750183
3504.181840	377337.033859	44.755188
3504.211926	377338.936889	44.760193
3504.096064	377335.699490	44.765197
3503.993061	377304.785709	44.770202
3504.062541	377308.768263	44.775207
3503.955787	377301.815767	44.780212
3503.895818	377310.956856	44.785217
3503.665020	377309.797939	44.790221
3503.693878	377305.367603	44.795226
3503.640800	377314.151498	44.800231
3503.782765	377310.415490	44.805236
3503.990900	377311.679910	44.810241
3503.840638	377308.880358	44.815245
3503.906244	377280.915914	44.820250
3503.532513	377271.309401	44.825255
3503.572839	377277.865605	44.830260
3504.029826	377270.798546	44.835265
3503.949920	377283.045987	44.840269
3503.940672	377275.213247	44.845274
3503.800918	377274.141680	44.850279
3504.202167	377279.674258	44.855284
3504.079949	377279.134075	44.860289
3504.303349	377282.481836	44.865293
3504.084830	377255.783219	44.870298
3503.840529	377249.869899	44.875303
3503.666998	377250.813117	44.880308
3504.340454	377249.816480	44.885313
3503.773575	377247.337146	44.890317
3504.357558	377250.805957	44.895322
3503.815329	377253.206443	44.900327
3503.845030	377235.523796	44.905332
3503.897992	377229.868712	44.910337
3503.635519	377221.236604	44.915341
3504.013918	377215.377453	44.920346
3503.951701	377230.445515	44.925351
3503.554309	377223.284590	44.930356
3503.750447	377221.295096	44.935361
3503.694648	377220.337436	44.940365
3503.629253	377229.504838	44.945370
3503.758560	377230.451053	44.950375
3503.835097	377225.631631	44.955380
3504.053946	377218.856570	44.960385
3503.576353	377235.516458	44.965389
3503.856767	377224.331232	44.970394
3503.855848	377232.242074	44.975399
3503.675150	377240.893544	44.980404
3503.972514	377216.631513	44.985409
3503.594962	377211.553206	44.990413
3503.758262	377213.308002	44.995418
3503.618877	377200.332302	45.000423
3503.657309	377203.454950	45.005428
3503.789389	377208.394189	45.010433
3503.543188	377205.991337	45.015437
3503.661157	377207.727864	45.020442
3503.775708	377207.709843	45.025447
3503.412340	377207.614759	45.030452
3503.858355	377207.086489	45.035457
3503.493196	377222.940090	45.040461
3503.156366	377223.603892	45.045466
3503.402613	377232.671154	45.050471
3503.558932	377250.044775	45.055476
3504.053134	377262.226899	45.060481
3503.610416	377268.274439	45.065485
3503.953319	377256.952163	45.070490
3503.906886	377244.953788	45.075495
3503.900896	377237.858170	45.080500
3504.170458	377229.879601	45.085505
3503.747182	377237.984391	45.090509
3504.115843	377235.535212	45.095514
3503.865710	377239.720917	45.100519
3504.061530	377243.886993	45.105524
3504.225331	377231.015990	45.110529
3503.669794	377221.438206	45.115533
3504.014551	377206.045855	45.120538
3503.590793	377199.753920	45.125543
3503.888230	377214.459898	45.130548
3503.878070	377211.790808	45.135553
3503.769643	377209.264432	45.140557
3504.051364	377219.419839	45.145562
3503.979620	377218.668188	45.150567
3503.888446	377208.279346	45.155572
3504.113403	377198.552734	45.160577
3503.868043	377197.396116	45.165581
3504.110413	377175.152203	45.170586
3503.714662	377177.478665	45.175591
3503.828637	377182.115536	45.180596
3504.140927	377178.098228	45.185601
3504.082188	377184.746417	45.190605
3504.147474	377177.436032	45.195610
3504.061405	377161.831976	45.200615
3503.736249	377146.698124	45.205620
3504.248082	377151.704515	45.210625
3503.959697	377143.254539	45.215629
3504.251162	377140.537761	45.220634
3504.129702	377152.715502	45.225639
3503.776947	377130.234977	45.230644
3503.783994	377119.143809	45.235649
3503.931104	377112.023966	45.240653
3503.874136	377111.575211	45.245658
3503.921393	377119.605639	45.250663
3503.784526	377102.814093	45.255668
3504.090847	377112.253427	45.260673
3504.059298	377116.150228	45.265677
3504.207965	377116.126814	45.270682
3504.169702	377089.857441	45.275687
3503.970095	377084.929039	45.280692
3503.863655	377086.955409	45.285697
3504.165622	377080.930269	45.290701
3503.978107	377088.565404	45.295706
3504.175324	377089.984174	45.300711
3504.261333	377079.007693	45.305716
3503.937395	377068.960846	45.310721
3503.560724	377066.960153	45.315725
3503.822017	377061.424727	45.320730
3504.019564	377060.452449	45.325735
3504.017610	377060.478282	45.330740
3504.107491	377061.914022	45.335745
3504.172098	377056.892976	45.340749
3503.971299	377033.599853	45.345754
3504.086358	377026.510498	45.350759
3503.840080	377017.290754	45.355764
3504.145555	377020.447508	45.360769
3503.863167	377022.450823	45.365773
3503.904202	377021.630467	45.370778
3503.985913	377017.166308	45.375783
3504.150813	377001.369897	45.380788
3504.361716	376990.246467	45.385793
3504.093863	376991.026549	45.390797
3503.917582	376995.505838	45.395802
3503.672389	376997.248913	45.400807
3503.841035	376983.970085	45.405812
3504.124301	376982.958817	45.410817
3503.465294	376972.583373	45.415821
3503.874313	376958.147343	45.420826
3504.068394	376958.015005	45.425831
3503.761553	376949.796832	45.430836
3503.723195	376951.405466	45.435841
3503.840760	376956.906627	45.440845
3503.687956	376953.547855	45.445850
3504.209881	376962.800523	45.450855
3503.809459	376967.162632	45.455860
3503.851590	376975.397389	45.460865
3503.803823	376972.352685	45.465869
3503.662183	376966.575710	45.470874
3503.955229	376966.504036	45.475879
3504.026531	376968.985600	45.480884
3503.692911	376947.137852	45.485889
3503.774594	376955.951394	45.490893
3504.396668	376945.195366	45.495898
3504.096470	376953.382501	45.500903
3503.906889	376947.129814	45.505908
3504.386594	376945.349840	45.510913
3503.647564	376933.944151	45.515917
3503.928819	376924.005084	45.520922
3503.704726	376908.906037	45.525927
3504.042270	376914.525045	45.530932
3503.979836	376909.752991	45.535937
3503.716851	376923.326732	45.540941
3504.349224	376912.721684	45.545946
3504.198445	376924.573459	45.550951
3504.074398	376912.307455	45.555956
3504.243541	376888.192678	45.560961
3503.980088	376884.825956	45.565965
3503.987828	376889.072676	45.570970
3504.232991	376887.177160	45.575975
3503.848740	376875.232079	45.580980
3503.923454	376866.241354	45.585985
3504.236832	376855.534103	45.590989
3504.141226	376837.362364	45.595994
3504.114445	376848.533215	45.600999
3504.001505	376852.213982	45.606004
3504.209708	376844.550272	45.611009
3503.637340	376833.372570	45.616013
3503.919110	376826.434879	45.621018
3504.225221	376820.434481	45.626023
3503.922561	376817.226570	45.631028
3503.880264	376812.196957	45.636033
3503.808936	376825.943923	45.641037
3503.973877	376825.841627	45.646042
3504.047546	376827.890409	45.651047
3503.776792	376826.763231	45.656052
3503.780611	376798.502983	45.661057
3503.778095	376794.967822	45.666061
3504.242465	376794.360336	45.671066
3503.982578	376787.482831	45.676071
3503.824823	376782.802139	45.681076
3503.991919	376781.325942	45.686081
3503.888931	376785.056014	45.691085
3504.178096	376782.670247	45.696090
3504.172595	376783.027314	45.701095
3503.651990	376764.642930	45.706100
3503.949348	376744.170628	45.711105
3503.810996	376756.732705	45.716109
3503.564693	376757.636566	45.721114
3503.752542	376747.406985	45.726119
3503.803118	376754.190582	45.731124
3503.960722	376765.205125	45.736129
3503.974631	376764.516233	45.741133
3503.942733	376745.622164	45.746138
3504.106436	376758.111053	45.751143
3503.683710	376752.149557	45.756148
3504.140641	376734.450021	45.761153
3504.062489	376728.281430	45.766157
3503.713996	376731.490719	45.771162
3503.610185	376730.795001	45.776167
3503.433442	376729.042485	45.781172
3503.731070	376727.698268	45.786177
3503.696531	376733.605051	45.791181
3503.639025	376731.452140	45.796186
3503.616982	376734.813312	45.801191
3503.309976	376735.039988	45.806196
3504.123719	376738.930377	45.811201
3503.758978	376745.957686	45.816205
3503.881782	376740.367800	45.821210
3503.683519	376744.748847	45.826215
3503.789212	376734.201578	45.831220
3504.449943	376734.834867	45.836225
3504.010320	376732.411692	45.841229
3504.223907	376714.699745	45.846234
3504.285910	376705.431194	45.851239
3503.985701	376704.181486	45.856244
3504.007399	376700.515307	45.861249
3504.037987	376710.481617	45.866253
3503.897471	376691.655566	45.871258
3503.940922	376684.653781	45.876263
3504.038647	376673.573591	45.881268
3504.047224	376674.030179	45.886273
3503.803628	376675.874760	45.891277
3504.051902	376671.155303	45.896282
3504.101666	376665.933064	45.901287
3503.823999	376674.650858	45.906292
3504.472994	376655.878033	45.911297
3504.045637	376650.629473	45.916301
3503.620189	376651.943204	45.921306
3503.989707	376645.042482	45.926311
3503.696753	376644.147736	45.931316
3504.052996	376642.234649	45.936321
3503.627923	376650.543332	45.941325
3503.692727	376651.525195	45.946330
3503.903315	376651.593738	45.951335
3503.860516	376649.845480	45.956340
3503.947012	376626.786504	45.961345
3503.556205	376617.843881	45.966349
3503.941163	376617.172637	45.971354
3504.086265	376611.833573	45.976359
3504.075921	376603.771948	45.981364
3503.961382	376610.505362	45.986369
3503.886836	376625.346671	45.991373
3503.743578	376614.457181	45.996378
3504.308206	376606.279223	46.001383
3503.954740	376603.155636	46.006388
3503.930197	376590.136147	46.011393
3503.652084	376592.596664	46.016397
3503.710461	376585.668810	46.021402
3503.733896	376589.455224	46.026407
3503.723244	376596.986183	46.031412
3504.062368	376591.387516	46.036417
3503.836606	376602.767947	46.041421
3503.605607	376590.569626	46.046426
3503.867815	376590.579135	46.051431
3503.739867	376591.159052	46.056436
3504.040220	376585.057784	46.061441
3504.061548	376581.951254	46.066445
3503.997368	376568.480169	46.071450
3504.138683	376567.618514	46.076455
3504.010348	376557.438869	46.081460
3504.044129	376556.263540	46.086465
3504.068512	376557.353541	46.091469
3503.951877	376564.112731	46.096474
3504.354010	376551.916054	46.101479
3503.506370	376536.788260	46.106484
3503.646528	376523.183110	46.111489
3504.031865	376534.543261	46.116493
3504.047996	376526.706364	46.121498
3503.953115	376526.975816	46.126503
3503.712602	376525.411428	46.131508
3504.401013	376521.919635	46.136513
3504.096611	376509.376782	46.141517
3503.503682	376497.210213	46.146522
3503.846400	376494.358107	46.151527
3503.837702	376495.148102	46.156532
3504.217783	376491.781358	46.161537
3503.865290	376490.336418	46.166541
3503.848446	376489.601510	46.171546
3503.956191	376492.331708	46.176551
3503.934171	376491.877420	46.181556
3503.962471	376494.594740	46.186561
3503.449385	376479.948203	46.191565
3503.620693	376480.913234	46.196570
3504.191012	376475.456057	46.201575
3503.787077	376477.580360	46.206580
3504.099914	376476.513532	46.211585
3504.095675	376488.825562	46.216589
3504.079351	376475.957356	46.221594
3504.179990	376473.067208	46.226599
3504.079780	376471.328019	46.231604
3504.160816	376448.346114	46.236609
3503.970420	376442.068041	46.241613
3503.864242	376439.286895	46.246618
3504.429366	376437.289904	46.251623
3503.720313	376430.890330	46.256628
3503.958062	376438.967090	46.261633
3503.636823	376428.614416	46.266637
3503.595655	376409.899711	46.271642
3503.554512	376412.577142	46.276647
3503.747624	376432.819631	46.281652
3504.067202	376414.607503	46.286657
3503.905700	376407.409140	46.291661
3503.748033	376413.309999	46.296666
3504.052898	376406.673823	46.301671
3503.801001	376405.340159	46.306676
3503.777722	376397.967324	46.311681
3503.738016	376405.401166	46.316685
3504.055840	376413.795947	46.321690
3503.675193	376414.670181	46.326695
3503.595719	376421.220027	46.331700
3503.992600	376410.677513	46.336705
3503.992663	376415.841212	46.341709
3503.766458	376391.966694	46.346714
3503.674152	376384.553896	46.351719
3503.634395	376375.046990	46.356724
3503.605734	376368.895956	46.361729
3503.337569	376377.714058	46.366733
3503.346917	376385.826936	46.371738
3503.913706	376403.364963	46.376743
3503.681325	376414.059706	46.381748
3503.704268	376390.858022	46.386753
3503.764670	376393.468528	46.391757
3503.863421	376389.027042	46.396762
3503.791451	376393.032050	46.401767
3503.864005	376389.205183	46.406772
3503.896075	376381.798158	46.411777
3503.407652	376398.485541	46.416781
3503.970047	376384.864467	46.421786
3504.296582	376392.036920	46.426791
3503.820749	376395.317239	46.431796
3504.013201	376391.980149	46.436801
3504.210615	376388.057234	46.441805
3503.833674	376378.272957	46.446810
3503.820088	376372.602836	46.451815
3503.823501	376362.605808	46.456820
3503.685695	376364.255623	46.461825
3503.762991	376363.327775	46.466829
3503.887340	376361.069785	46.471834
3504.115587	376357.701597	46.476839
3503.875654	376362.191019	46.481844
3503.953404	376366.248670	46.486849
3503.788509	376361.670804	46.491853
3504.184108	376339.834628	46.496858
3504.008152	376334.368226	46.501863
3503.746568	376321.869420	46.506868
3503.974216	376321.299351	46.511873
3503.500053	376323.943497	46.516877
3503.381657	376324.547344	46.521882
3503.893204	376323.678028	46.526887
3503.519646	376333.352209	46.531892
3503.640000	376328.322259	46.536897
3503.766424	376324.181631	46.541901
3504.166669	376327.450641	46.546906
3503.994319	376328.495440	46.551911
3504.010416	376332.054109	46.556916
3504.088054	376326.827419	46.561921
3503.593227	376311.618328	46.566925
3503.815926	376297.745687	46.571930
3503.831354	376293.495419	46.576935
3503.732976	376308.518669	46.581940
3503.777449	376297.446795	46.586945
3503.468752	376299.606925	46.591949
3503.545173	376303.156060	46.596954
3503.722524	376303.789463	46.601959
3503.351490	376305.857701	46.606964
3503.895663	376297.784661	46.611969
3503.693906	376310.611267	46.616973
3503.824569	376310.132840	46.621978
3503.958749	376299.911630	46.626983
3503.777699	376309.097525	46.631988
3503.647855	376309.397943	46.636993
3503.838536	376310.003802	46.641997
3503.661129	376313.669373	46.647002
3503.978949	376311.355359	46.652007
3503.717222	376326.175496	46.657012
3503.836511	376318.347686	46.662017
3503.510600	376318.857156	46.667021
3503.748277	376321.999247	46.672026
3504.010008	376312.648158	46.677031
3503.782151	376303.883196	46.682036
3503.910732	376286.387993	46.687041
3503.969496	376295.892092	46.692045
3503.726235	376283.364940	46.697050
3503.985310	376281.187394	46.702055
3503.668589	376286.680992	46.707060
3504.016242	376285.176233	46.712065
3503.754090	376287.405315	46.717069
3503.777985	376300.577800	46.722074
3504.408124	376287.683646	46.727079
3503.681576	376279.429939	46.732084
3503.597643	376263.112971	46.737089
3503.687672	376261.801557	46.742093
3503.812543	376249.928424	46.747098
3504.144402	376257.227243	46.752103
3503.641534	376262.394159	46.757108
3504.000981	376253.103918	46.762113
3503.870985	376262.459809	46.767117
3503.937883	376264.051830	46.772122
3504.067415	376269.067897	46.777127
3503.822825	376267.376960	46.782132
3503.984100	376248.248627	46.787137
3503.834758	376244.685755	46.792141
3503.499122	376237.871004	46.797146
3503.976589	376225.611446	46.802151
3503.827634	376232.808224	46.807156
3504.089538	376225.085033	46.812161
3504.068588	376234.983298	46.817165
3503.590583	376237.144760	46.822170
3504.230890	376223.969175	46.827175
3504.155382	376223.879454	46.832180
3504.309549	376213.629626	46.837185
3503.949127	376202.138438	46.842189
3504.127049	376196.234523	46.847194
3504.124253	376195.014092	46.852199
3503.704426	376202.940488	46.857204
3504.263198	376188.505946	46.862209
3504.089812	376164.648380	46.867213
3503.989945	376161.128553	46.872218
3503.889242	376152.572388	46.877223
3503.977270	376154.924175	46.882228
3504.132683	376147.828286	46.887233
3504.022240	376145.836333	46.892237
3504.119874	376153.172199	46.897242
3504.266440	376133.639149	46.902247
3504.091635	376133.361631	46.907252
3504.071401	376111.921748	46.912257
3503.973713	376122.747894	46.917261
3503.896832	376112.763497	46.922266
3504.042162	376108.340054	46.927271
3503.885924	376103.252055	46.932276
3503.910086	376085.137353	46.937281
3503.948093	376104.030943	46.942285
3504.158353	376088.837486	46.947290
3503.927198	376092.002838	46.952295
3503.937036	376098.742111	46.957300
3504.219950	376089.438495	46.962305
3503.926215	376071.450353	46.967309
3503.916270	376063.413994	46.972314
3504.245050	376050.796337	46.977319
3503.786164	376061.806785	46.982324
3504.057390	376050.673559	46.987329
3503.836423	376061.722706	46.992333
3503.759266	376064.761968	46.997338
3503.950801	376055.879778	47.002343
3503.861833	376061.057597	47.007348
3503.783318	376040.313683	47.012353
3504.159152	376034.556515	47.017357
3504.028074	376035.467613	47.022362
3504.101650	376021.898257	47.027367
3503.937879	376041.459694	47.032372
3503.853739	376034.910392	47.037377
3503.824204	376033.236321	47.042381
3504.006907	376032.062870	47.047386
3504.234633	376012.466058	47.052391
3503.788194	376006.508199	47.057396
3503.670934	375997.827434	47.062401
3503.884606	376010.868265	47.067405
3503.851410	376003.395179	47.072410
3504.095184	375999.821013	47.077415
3503.706072	375997.135439	47.082420
3503.874688	375988.943652	47.087425
3503.636177	375995.060846	47.092429
3503.678482	376001.769566	47.097434
3503.710676	376007.411537	47.102439
3503.632530	375997.452748	47.107444
3503.960933	376003.683813	47.112449
3504.040125	375986.018230	47.117453
3503.915582	375976.397450	47.122458
3503.643096	375967.181608	47.127463
3503.504250	375964.736273	47.132468
3503.709871	375962.872403	47.137473
3503.843587	375972.262981	47.142477
3503.575986	375964.470829	47.147482
3504.170051	375958.958956	47.152487
3503.639040	375973.363930	47.157492
3503.678028	375966.820588	47.162497
3504.018180	375967.224765	47.167501
3503.760767	375978.661248	47.172506
3503.780573	375974.079576	47.177511
3503.786717	375980.743143	47.182516
3503.653691	375973.260396	47.187521
3503.381794	375980.171412	47.192525
3503.508629	375970.994190	47.197530
3503.886909	375976.657764	47.202535
3503.766239	375981.967789	47.207540
3503.926797	375982.832784	47.212545
3504.119935	375975.934396	47.217549
3503.696417	375960.459531	47.222554
3503.689239	375943.189136	47.227559
3503.375343	375949.445439	47.232564
3503.748438	375933.971813	47.237569
3503.766372	375933.485766	47.242573
3503.611105	375938.903014	47.247578
3503.906011	375939.161723	47.252583
3503.565897	375941.021596	47.257588
3503.460740	375937.324528	47.262593
3503.859640	375942.628731	47.267597
3503.583325	375953.712093	47.272602
3503.611573	375953.987521	47.277607
3503.822808	375956.854015	47.282612
3503.984898	375949.095679	47.287617
3503.609618	375960.118374	47.292621
3503.673156	375964.280059	47.297626
3504.117355	375949.481993	47.302631
3503.868217	375957.203394	47.307636
3503.652189	375963.291602	47.312641
3503.870545	375957.889997	47.317645
3503.874167	375963.332997	47.322650
3503.735613	375959.183347	47.327655
3503.581424	375962.336542	47.332660
3503.909443	375965.998553	47.337665
3503.644636	375935.694347	47.342669
3503.584719	375924.588000	47.347674
3503.657995	375925.339610	47.352679
3503.447272	375929.061356	47.357684
3503.573283	375941.302088	47.362689
3504.001649	375950.493470	47.367693
3503.680829	375942.658853	47.372698
3504.061716	375938.070968	47.377703
3503.970012	375938.568854	47.382708
3504.230166	375922.782399	47.387713
3504.064173	375932.474736	47.392717
3503.709991	375935.481492	47.397722
3503.999604	375927.372312	47.402727
3503.992169	375931.290852	47.407732
3503.849163	375920.019581	47.412737
3504.122803	375905.858947	47.417741
3503.959623	375901.204447	47.422746
3504.473171	375882.808794	47.427751
3503.969917	375894.233292	47.432756
3503.972614	375887.212374	47.437761
3503.854072	375884.255086	47.442765
3503.759202	375880.098523	47.447770
3504.210615	375863.823946	47.452775
3504.007520	375863.550898	47.457780
3503.680281	375863.551845	47.462785
3503.893375	375867.384655	47.467789
3504.090934	375861.350403	47.472794
3504.214613	375856.955791	47.477799
3503.999573	375859.024827	47.482804
3504.073453	375847.515754	47.487809
3504.188140	375832.795175	47.492813
3504.000875	375820.513396	47.497818
3504.038864	375825.569427	47.502823
3503.885529	375836.251826	47.507828
3504.148357	375823.975205	47.512833
3504.291430	375807.215175	47.517837
3503.945036	375795.899712	47.522842
3503.966704	375785.975966	47.527847
3503.879865	375799.903791	47.532852
3503.861575	375798.838419	47.537857
3504.034127	375794.766755	47.542861
3503.889329	375796.926438	47.547866
3503.840563	375765.773969	47.552871
3504.180212	375766.941337	47.557876
3503.559236	375756.305195	47.562881
3504.067462	375759.836988	47.567885
3503.624056	375756.218814	47.572890
3503.727797	375749.258209	47.577895
3503.679714	375760.559913	47.582900
3503.794574	375758.812129	47.587905
3503.888756	375770.116777	47.592909
3503.856008	375765.746885	47.597914
3503.920543	375755.790918	47.602919
3503.828492	375778.876882	47.607924
3504.129564	375757.818445	47.612929
3503.728949	375747.350960	47.617933
3503.696967	375728.583614	47.622938
3504.249681	375717.024243	47.627943
3503.806647	375723.555365	47.632948
3503.869179	375720.416818	47.637953
3504.503704	375736.799762	47.642957
3504.017448	375730.034173	47.647962
3504.059425	375707.617636	47.652967
3504.075921	375699.856831	47.657972
3504.033130	375685.491775	47.662977
3503.905319	375694.058904	47.667981
3503.837001	375693.789985	47.672986
3504.131562	375681.966171	47.677991
3504.068992	375691.896585	47.682996
3503.776864	375680.928630	47.688001
3503.568438	375653.438808	47.693005
3503.576439	375652.878017	47.698010
3503.761122	375648.702672	47.703015
3503.998739	375656.347180	47.708020
3504.083047	375646.057379	47.713025
3503.642008	375650.197116	47.718029
3503.692337	375659.244831	47.723034
3503.728883	375657.662046	47.728039
3503.589304	375658.218378	47.733044
3503.611429	375663.989174	47.738049
3503.592656	375663.025623	47.743053
3503.711591	375664.558567	47.748058
3503.641885	375668.283481	47.753063
3503.635696	375675.356039	47.758068
3503.991879	375663.446167	47.763073
3503.877351	375665.753693	47.768077
3503.691437	375672.854664	47.773082
3503.876356	375662.650710	47.778087
3504.039224	375666.949345	47.783092
3503.660672	375679.778662	47.788097
3503.789190	375673.093934	47.793101
3503.922870	375657.327371	47.798106
3503.916746	375644.762533	47.803111
3503.886485	375656.163196	47.808116
3503.819421	375640.759043	47.813121
3503.972810	375635.469415	47.818125
3503.875380	375642.123973	47.823130
3504.144772	375640.071948	47.828135
3504.015984	375641.923863	47.833140
3503.617555	375647.684835	47.838145
3503.635058	375638.397637	47.843149
3503.883544	375642.809924	47.848154
3503.718568	375635.204981	47.853159
3503.531986	375619.997774	47.858164
3503.588183	375618.895185	47.863169
3503.716712	375621.647593	47.868173
3503.419111	375624.645426	47.873178
3504.048901	375633.703289	47.878183
3504.246601	375614.848706	47.883188
3503.823437	375610.184399	47.888193
3504.016984	375607.076006	47.893197
3503.854327	375604.151109	47.898202
3503.868518	375609.338114	47.903207
3504.204142	375607.148431	47.908212
3504.035541	375607.556729	47.913217
3503.891420	375587.891312	47.918221
3503.481385	375583.504734	47.923226
3503.746836	375572.295979	47.928231
3503.849178	375571.236968	47.933236
3503.534176	375581.690620	47.938241
3503.606243	375578.601429	47.943245
3503.817470	375565.722398	47.948250
3504.082435	375577.941273	47.953255
3504.200348	375577.871846	47.958260
3504.262619	375579.540938	47.963265
3504.216205	375564.362425	47.968269
3503.597211	375562.069282	47.973274
3503.908177	375544.926483	47.978279
3504.021414	375536.183743	47.983284
3503.644297	375539.906393	47.988289
3504.020321	375541.424136	47.993293
3503.530564	375538.703568	47.998298
3503.944683	375536.704969	48.003303
3503.561576	375554.546155	48.008308
3503.786648	375550.313541	48.013313
3503.841759	375552.746878	48.018317
3503.794761	375554.840238	48.023322
3503.769944	375540.345104	48.028327
3503.766792	375551.639762	48.033332
3503.446638	375555.404279	48.038337
3503.753141	375550.064997	48.043341
3503.683113	375549.236732	48.048346
3503.964056	375541.027097	48.053351
3503.735474	375551.009227	48.058356
3503.763922	375542.788636	48.063361
3503.882877	375532.315268	48.068365
3503.704892	375526.772767	48.073370
3503.746768	375521.526190	48.078375
3504.041901	375528.373079	48.083380
3503.749566	375527.172963	48.088385
3503.686196	375523.189443	48.093389
3503.546223	375531.275224	48.098394
3503.722956	375532.213983	48.103399
3504.037008	375528.043611	48.108404
3503.817088	375533.725505	48.113409
3503.700275	375525.629622	48.118413
3503.823711	375522.862988	48.123418
3503.809843	375516.989295	48.128423
3503.944275	375534.748672	48.133428
3504.060477	375534.119900	48.138433
3504.008386	375519.349262	48.143437
3503.744089	375512.853793	48.148442
3504.115648	375489.621919	48.153447
3503.806583	375498.014246	48.158452
3503.861033	375499.557391	48.163457
3504.170298	375488.774119	48.168461
3503.906555	375498.456575	48.173466
3503.836368	375493.456644	48.178471
3503.534176	375493.326446	48.183476
3503.737842	375495.685427	48.188481
3503.871658	375510.595954	48.193485
3503.651078	375498.370219	48.198490
3503.901845	375468.442026	48.203495
3503.476865	375472.833614	48.208500
3503.709785	375461.121229	48.213505
3503.664779	375467.131599	48.218509
3503.675656	375464.102947	48.223514
3503.943756	375455.183086	48.228519
3503.497905	375451.488958	48.233524
3503.622142	375462.636318	48.238529
3504.000430	375469.546382	48.243533
3503.658778	375469.956601	48.248538
3503.906019	375462.388208	48.253543
3503.753380	375470.755811	48.258548
3504.132316	375472.273097	48.263553
3504.161894	375469.902855	48.268557
3503.718438	375483.378423	48.273562
3503.811357	375474.537134	48.278567
3503.689249	375478.244911	48.283572
3503.801600	375470.214538	48.288577
3503.576276	375452.571427	48.293581
3503.833402	375447.672369	48.298586
3504.113034	375416.238782	48.303591
3503.816854	375437.881853	48.308596
3503.706850	375443.419197	48.313601
3503.726949	375431.460639	48.318605
3503.367580	375430.983359	48.323610
3503.779318	375437.633769	48.328615
3503.906508	375447.457933	48.333620
3503.819045	375442.791410	48.338625
3503.950651	375451.597388	48.343629
3503.429069	375456.131434	48.348634
3503.547548	375450.160498	48.353639
3503.849665	375457.769409	48.358644
3503.245909	375453.820436	48.363649
3503.900153	375449.774337	48.368653
3503.878310	375455.984545	48.373658
3504.130799	375453.070319	48.378663
3504.009170	375457.312203	48.383668
3504.059580	375444.178748	48.388673
3503.743169	375430.925219	48.393677
3503.624294	375436.667463	48.398682
3503.695557	375431.645163	48.403687
3503.764646	375425.503971	48.408692
3503.739068	375432.961194	48.413697
3503.922284	375420.925972	48.418701
3503.663256	375429.768272	48.423706
3503.788110	375429.265316	48.428711
3503.808867	375427.023652	48.433716
3503.629481	375430.536992	48.438721
3504.025584	375427.472875	48.443725
3503.717121	375443.776078	48.448730
3504.029707	375422.919145	48.453735
3503.630944	375431.707224	48.458740
3503.775035	375425.376114	48.463745
3504.151357	375432.744365	48.468749
3503.918026	375412.736845	48.473754
3504.124688	375403.623187	48.478759
3504.117697	375388.591000	48.483764
3503.556392	375401.627355	48.488769
3503.596934	375399.662371	48.493773
3503.664374	375396.650209	48.498778
3503.960415	375398.969155	48.503783
3504.055088	375391.882737	48.508788
3503.943169	375411.665215	48.513793
3504.130890	375400.366953	48.518797
3503.942346	375384.981908	48.523802
3504.003415	375364.520828	48.528807
3503.888689	375360.825220	48.533812
3503.816577	375371.978207	48.538817
3503.801956	375358.422572	48.543821
3503.792953	375368.497220	48.548826
3503.932045	375357.766253	48.553831
3503.955916	375372.236341	48.558836
3503.557331	375364.998962	48.563841
3504.282881	375361.323139	48.568845
3504.079518	375350.112126	48.573850
3503.610262	375330.828668	48.578855
3503.953975	375339.702888	48.583860
3503.986590	375330.209733	48.588865
3503.996236	375321.483324	48.593869
3503.603208	375339.860354	48.598874
3503.786794	375318.438705	48.603879
3503.856094	375330.256153	48.608884
3503.786939	375339.450014	48.613889
3503.932186	375326.326966	48.618893
3503.753618	375343.728913	48.623898
3503.849865	375329.214565	48.628903
3503.831120	375297.955243	48.633908
3503.735759	375300.844816	48.638913
3504.225809	375287.794432	48.643917
3503.589539	375294.661418	48.648922
3503.688519	375293.653806	48.653927
3503.883683	375301.330529	48.658932
3503.647679	375297.348841	48.663937
3503.816958	375289.411181	48.668941
3503.791510	375308.645856	48.673946
3503.845571	375305.737552	48.678951
3504.012434	375298.309021	48.683956
3503.715497	375307.233652	48.688961
3504.283866	375304.727350	48.693965
3503.856433	375284.470642	48.698970
3503.822352	375277.709806	48.703975
3504.032547	375261.981868	48.708980
3503.873443	375266.280571	48.713985
3504.054541	375260.604955	48.718989
3504.024259	375261.322074	48.723994
3504.154232	375261.886672	48.728999
3503.826112	375267.636582	48.734004
3503.665078	375249.016603	48.739009
3504.050039	375227.537634	48.744013
3503.893531	375231.683306	48.749018
3503.951856	375222.313248	48.754023
3503.943365	375230.352865	48.759028
3503.832435	375234.771142	48.764033
3503.997364	375230.904126	48.769037
3503.787346	375225.366648	48.774042
3503.952243	375224.068803	48.779047
3503.470932	375223.051177	48.784052
3503.783914	375228.063809	48.789057
3504.082527	375220.182001	48.794061
3503.837946	375205.874114	48.799066
3503.723251	375202.763545	48.804071
3503.724380	375190.553542	48.809076
3503.679597	375186.770549	48.814081
3503.863223	375189.870399	48.819085
3503.576654	375204.516810	48.824090
3503.978212	375193.184686	48.829095
3504.117915	375200.437762	48.834100
3503.844897	375202.744932	48.839105
3504.040067	375189.613948	48.844109
3503.877919	375204.825748	48.849114
3503.783819	375202.653103	48.854119
3504.079556	375174.549072	48.859124
3504.178268	375173.948497	48.864129
3503.865386	375169.215830	48.869133
3503.781116	375162.233973	48.874138
3504.064269	375165.801400	48.879143
3504.101045	375167.652600	48.884148
3503.869726	375153.418909	48.889153
3503.998537	375145.029747	48.894157
3503.762983	375135.324567	48.899162
3503.561367	375132.812793	48.904167
3503.674796	375128.190788	48.909172
3503.588261	375132.834156	48.914177
3504.073363	375129.170887	48.919181
3503.982537	375122.037436	48.924186
3503.635220	375126.620281	48.929191
3503.846918	375130.046384	48.934196
3503.734673	375145.911688	48.939201
3503.946704	375129.293102	48.944205
3503.805183	375140.355375	48.949210
3503.938076	375128.302585	48.954215
3504.156265	375137.018631	48.959220
3503.935603	375110.420685	48.964225
3504.181581	375105.396162	48.969229
3503.947772	375110.062814	48.974234
3503.926310	375091.115450	48.979239
3503.855709	375105.651442	48.984244
3503.730275	375111.878079	48.989249
3503.903259	375096.435772	48.994253
3503.668538	375106.266356	48.999258
3503.991289	375108.453911	49.004263
3503.872654	375081.687192	49.009268
3503.518478	375055.695377	49.014273
3503.786949	375054.406590	49.019277
3503.509730	375063.709718	49.024282
3503.738839	375063.444650	49.029287
3503.858200	375057.397205	49.034292
3503.458699	375055.959643	49.039297
3503.793839	375053.871757	49.044301
3504.067315	375058.865218	49.049306
3503.768491	375060.565978	49.054311
3503.727521	375070.544004	49.059316
3503.644318	375068.878377	49.064321
3503.846995	375063.911569	49.069325
3503.617646	375068.755583	49.074330
3503.813748	375066.816865	49.079335
3503.772695	375065.577011	49.084340
3503.634519	375070.940797	49.089345
3503.888875	375070.239302	49.094349
3503.638688	375072.619183	49.099354
3503.912427	375069.650695	49.104359
3503.636376	375067.099810	49.109364
3503.894254	375073.036918	49.114369
3503.916913	375072.957113	49.119373
3503.720357	375058.997705	49.124378
3503.622192	375049.118161	49.129383
3503.922070	375041.210682	49.134388
3503.646638	375040.872751	49.139393
3503.657266	375035.071429	49.144397
3503.403214	375043.938463	49.149402
3503.250923	375038.544457	49.154407
3503.524076	375050.329760	49.159412
3503.535046	375071.110471	49.164417
3503.767282	375071.150158	49.169421
3503.194393	375079.050093	49.174426
3503.348598	375081.976541	49.179431
3503.784201	375090.912600	49.184436
3503.557909	375087.972288	49.189441
3504.057139	375078.659682	49.194445
3503.886322	375076.753533	49.199450
3503.921449	375081.733797	49.204455
3503.918108	375071.254208	49.209460
3503.674103	375055.445370	49.214465
3503.799779	375053.695847	49.219469
3503.773546	375067.817840	49.224474
3503.704348	375053.126050	49.229479
3503.745593	375064.591886	49.234484
3503.316798	375067.203502	49.239489
3503.667386	375055.574149	49.244493
3503.617258	375069.343796	49.249498
3503.615291	375068.759135	49.254503
3503.921370	375059.019186	49.259508
3503.447650	375066.038575	49.264513
3503.839147	375059.235860	49.269517
3503.823910	375054.176314	49.274522
3504.038911	375064.571748	49.279527
3504.031379	375062.334536	49.284532
3503.823345	375064.504254	49.289537
3503.870773	375065.972214	49.294541
3503.900177	375067.646522	49.299546
3503.987548	375057.127151	49.304551
3503.791493	375039.886232	49.309556
3503.473156	375032.076484	49.314561
3503.862046	375024.180367	49.319565
3503.506564	375027.899642	49.324570
3503.435704	375038.416587	49.329575
3503.896724	375026.489956	49.334580
3503.706933	375022.450060	49.339585
3503.633842	375021.851205	49.344589
3503.636322	375029.024255	49.349594
3503.849618	375029.397622	49.354599
3503.958457	375018.493286	49.359604
3503.828730	375033.114964	49.364609
3503.854999	375021.892996	49.369613
3503.435370	375033.304514	49.374618
3503.696759	375025.097867	49.379623
3503.815223	375021.670613	49.384628
3503.962294	375032.254856	49.389633
3503.977098	375020.754889	49.394637
3503.981677	375030.420474	49.399642
3503.883427	375018.149819	49.404647
3503.698471	375012.455724	49.409652
3503.401740	375003.421558	49.414657
3503.890589	375004.794299	49.419661
3503.710982	374997.929235	49.424666
3503.684152	375000.350122	49.429671
3503.898763	375000.621532	49.434676
3503.668600	374990.940903	49.439681
3504.054814	374988.361629	49.444685
3503.395713	375003.982753	49.449690
3503.970853	374995.624750	49.454695
3503.900287	374989.938007	49.459700
3503.635033	374999.391883	49.464705
3503.455821	374993.188129	49.469709
3503.690228	374991.828413	49.474714
3503.414209	374998.053435	49.479719
3503.634704	374999.494038	49.484724
3503.513288	375001.522878	49.489729
3503.601006	374999.931978	49.494733
3503.654131	375006.003215	49.499738
3503.775641	374991.026879	49.504743
3503.819879	375003.001009	49.509748
3503.517447	375012.689696	49.514753
3504.001179	374992.822985	49.519757
3503.897494	375007.694930	49.524762
3503.470894	375001.937286	49.529767
3503.851033	374996.586291	49.534772
3504.081547	374997.974434	49.539777
3504.076415	374997.771834	49.544781
3503.686712	374988.421676	49.549786
3503.511831	374984.481169	49.554791
3503.667274	374974.815889	49.559796
3503.631512	374973.753258	49.564801
3504.105442	374973.780173	49.569805
3503.955744	374980.214165	49.574810
3503.855596	374965.145674	49.579815
3504.025060	374973.945770	49.584820
3504.002948	374963.545433	49.589825
3504.123104	374969.529767	49.594829
3504.067154	374963.128460	49.599834
3503.943290	374962.563068	49.604839
3504.043858	374937.720287	49.609844
3503.486374	374938.037444	49.614849
3504.145846	374930.480096	49.619853
3503.853546	374940.574198	49.624858
3504.022912	374948.891003	49.629863
3504.044179	374936.423366	49.634868
3503.737939	374939.905927	49.639873
3503.903942	374934.410714	49.644877
3503.807509	374941.446792	49.649882
3503.631478	374929.162968	49.654887
3503.707726	374908.394011	49.659892
3503.615650	374915.760091	49.664897
3503.479282	374905.148864	49.669901
3503.721496	374925.994842	49.674906
3503.465460	374932.827215	49.679911
3503.947846	374918.149927	49.684916
3503.519054	374931.470733	49.689921
3503.980391	374916.542397	49.694925
3503.754581	374910.981934	49.699930
3503.830841	374919.186277	49.704935
3503.763256	374907.724740	49.709940
3503.696382	374910.940525	49.714945
3503.721248	374917.601305	49.719949
3504.007697	374912.392298	49.724954
3503.655262	374904.562479	49.729959
3504.103329	374919.194605	49.734964
3503.622895	374921.890705	49.739969
3504.041404	374908.826074	49.744973
3503.520295	374920.838727	49.749978
3503.757489	374909.583384	49.754983
3504.056173	374917.981501	49.759988
3503.535778	374918.826983	49.764993
3504.019301	374911.882509	49.769997
3504.057030	374895.901883	49.775002
3503.887029	374882.675905	49.780007
3504.127855	374873.480416	49.785012
3503.946406	374882.641257	49.790017
3503.704897	374883.849651	49.795021
3503.538318	374883.087510	49.800026
3503.720530	374880.133479	49.805031
3503.955586	374881.571783	49.810036
3503.822179	374891.055716	49.815041
3503.693984	374885.708756	49.820045
3503.859817	374877.949624	49.825050
3503.480506	374878.696490	49.830055
3503.738794	374888.423750	49.835060
3503.596422	374885.648220	49.840065
3503.763028	374871.046273	49.845069
3503.716079	374887.562731	49.850074
3503.657314	374864.627469	49.855079
3503.755855	374850.417839	49.860084
3503.616646	374850.414497	49.865089
3503.651065	374831.254677	49.870093
3503.611808	374849.983000	49.875098
3503.511625	374843.792168	49.880103
3504.013514	374851.878362	49.885108
3503.448665	374842.555858	49.890113
3503.813724	374851.859248	49.895117
3503.839145	374848.853688	49.900122
3503.226372	374859.201974	49.905127
3503.606640	374842.938238	49.910132
3503.555119	374858.819491	49.915137
3504.009035	374860.808261	49.920141
3503.829316	374856.003630	49.925146
3503.668876	374861.065713	49.930151
3503.889052	374857.317115	49.935156
3503.770477	374860.083201	49.940161
3504.199816	374853.299908	49.945165
3503.995348	374851.958694	49.950170
3503.804603	374865.750639	49.955175
3504.065724	374863.623570	49.960180
3503.764375	374855.912853	49.965185
3503.706370	374831.196825	49.970189
3503.639556	374824.237588	49.975194
3503.857822	374828.425804	49.980199
3503.971058	374819.682912	49.985204
3503.854253	374833.005303	49.990209
3503.795176	374820.626645	49.995213
3504.260237	374834.721926	50.000218
3503.751120	374816.589216	50.005223
3504.090238	374825.489711	50.010228
3503.851682	374831.047460	50.015233
3503.888633	374831.372395	50.020237
3504.013020	374802.582946	50.025242
3503.800086	374792.009232	50.030247
3503.636052	374788.652056	50.035252
3503.487464	374790.252763	50.040257
3503.581806	374785.557424	50.045261
3503.771208	374788.096765	50.050266
3503.511911	374800.500503	50.055271
3503.786312	374789.595371	50.060276
3503.601763	374805.345049	50.065281
3503.917784	374794.407901	50.070285
3503.485167	374795.875447	50.075290
3503.614638	374794.049000	50.080295
3503.918247	374796.875537	50.085300
3503.878374	374807.082391	50.090305
3504.082620	374798.477732	50.095309
3503.695608	374801.438885	50.100314
3504.004058	374793.148440	50.105319
3504.260923	374798.729623	50.110324
3503.912657	374792.145563	50.115329
3503.815938	374765.578673	50.120333
3503.711382	374761.601590	50.125338
3503.846526	374771.348346	50.130343
3503.718592	374755.521043	50.135348
3503.486230	374760.518195	50.140353
3503.614505	374766.806526	50.145357
3503.961993	374761.765913	50.150362
3503.591023	374767.522667	50.155367
3503.861691	374760.382879	50.160372
3503.767878	374765.968630	50.165377
3504.017413	374764.377577	50.170381
3503.903520	374766.354364	50.175386
3503.996498	374758.683040	50.180391
3503.998954	374767.153457	50.185396
3503.798682	374756.933858	50.190401
3503.922709	374729.950484	50.195405
3503.828956	374736.706359	50.200410
3503.716192	374736.342710	50.205415
3503.853244	374729.961731	50.210420
3503.897527	374734.304649	50.215425
3503.889317	374731.202647	50.220429
3503.927215	374723.158460	50.225434
3503.573443	374741.936553	50.230439
3503.869703	374729.425380	50.235444
3503.490950	374734.369366	50.240449
3503.610887	374740.684456	50.245453
3503.833050	374741.488864	50.250458
3503.699514	374741.713564	50.255463
3503.681191	374723.681286	50.260468
3503.488915	374740.424278	50.265473
3503.497070	374733.325986	50.270477
3503.787802	374746.838354	50.275482
3503.379269	374747.742468	50.280487
3503.864925	374734.412790	50.285492
3503.693919	374736.576671	50.290497
3503.629628	374742.183195	50.295501
3503.946256	374735.366826	50.300506
3503.426667	374743.818026	50.305511
3503.945773	374741.573854	50.310516
3503.842252	374751.154844	50.315521
3503.814521	374734.141562	50.320525
3503.644296	374719.363873	50.325530
3503.472773	374721.680462	50.330535
3504.106813	374703.494170	50.335540
3503.750220	374709.528472	50.340545
3503.903443	374709.529775	50.345549
3504.124643	374704.229307	50.350554
3503.945943	374713.008187	50.355559
3504.012431	374719.001042	50.360564
3503.645275	374715.828596	50.365569
3504.082570	374711.486033	50.370573
3503.668223	374716.155834	50.375578
3503.836164	374706.463077	50.380583
3503.682206	374679.014864	50.385588
3503.395045	374686.996892	50.390593
3503.911319	374685.261917	50.395597
3503.901585	374678.166443	50.400602
3503.498419	374680.392467	50.405607
3504.044994	374676.236125	50.410612
3503.631249	374680.626021	50.415617
3503.857086	374673.340679	50.420621
3503.800868	374673.018966	50.425626
3503.681306	374682.322694	50.430631
3503.891511	374673.513566	50.435636
3503.896782	374681.500240	50.440641
3503.824547	374679.603925	50.445645
3503.940951	374681.188182	50.450650
3503.717533	374682.088470	50.455655
3504.113828	374691.336083	50.460660
3503.751016	374670.865354	50.465665
3503.773759	374653.640558	50.470669
3503.737011	374644.616087	50.475674
3503.355326	374650.221925	50.480679
3503.554999	374646.654613	50.485684
3503.287451	374650.131082	50.490689
3503.572151	374662.067297	50.495693
3503.859314	374679.726588	50.500698
3504.025051	374679.675037	50.505703
3503.808877	374668.338674	50.510708
3503.640093	374669.026824	50.515713
3503.778140	374649.163721	50.520717
3503.793166	374653.714774	50.525722
3503.732530	374646.220340	50.530727
3503.955841	374649.695522	50.535732
3503.859099	374624.425865	50.540737
3503.915875	374606.686916	50.545741
3503.542039	374553.759375	50.550746
3503.399831	374520.483960	50.555751
3503.320178	374447.261331	50.560756
3502.839300	374387.609484	50.565761
3503.182626	374308.825171	50.570765
3503.046444	374221.671123	50.575770
3502.381507	374141.519610	50.580775
3502.185441	374039.213610	50.585780
3502.014729	373955.218774	50.590785
3501.641213	373826.815380	50.595789
3501.248189	373719.146834	50.600794
3500.741485	373593.383908	50.605799
3500.731506	373456.196553	50.610804
3500.081787	373346.074657	50.615809
3499.743913	373199.602377	50.620813
3499.121121	373056.252699	50.625818
3498.741405	372920.241330	50.630823
3498.462121	372771.977576	50.635828
3497.822281	372634.301999	50.640833
3497.243265	372476.952022	50.645837
3497.034477	372322.722810	50.650842
3496.327523	372159.439123	50.655847
3495.870620	371991.027415	50.660852
3495.599097	371826.605151	50.665857
3495.293894	371657.125115	50.670861
3494.765762	371483.202277	50.675866
3493.843364	371296.595768	50.680871
3493.414326	371137.029273	50.685876
3492.516285	370963.951422	50.690881
3492.192563	370785.363352	50.695885
3491.706579	370594.868774	50.700890
3491.110012	370415.635412	50.705895
3490.961485	370218.649435	50.710900
3490.244194	370049.660646	50.715905
3489.785609	369851.068375	50.720909
3489.038841	369649.238904	50.725914
3487.951343	369450.693339	50.730919
3487.650550	369267.007183	50.735924
3487.033268	369070.039195	50.740929
3486.549508	368871.802590	50.745933
3486.032729	368680.744735	50.750938
3485.376610	368475.206499	50.755943
3485.281915	368258.435169	50.760948
3484.366489	368067.056039	50.765953
3483.743800	367857.515294	50.770957
3482.847198	367640.155328	50.775962
3482.077066	367439.769531	50.780967
3481.904609	367229.289598	50.785972
3481.228175	367020.542089	50.790977
3480.666481	366811.877230	50.795981
3480.159004	366604.882023	50.800986
3479.320400	366390.432653	50.805991
3478.682816	366165.697073	50.810996
3477.890510	365954.215093	50.816001
3477.231146	365744.848305	50.821005
3476.553685	365527.621507	50.826010
3475.752619	365325.653662	50.831015
3475.084878	365109.466490	50.836020
3474.685087	364889.953726	50.841025
3473.992281	364673.946551	50.846029
3473.442769	364458.857113	50.851034
3472.304021	364245.564556	50.856039
3471.630371	364033.953102	50.861044
3471.110754	363821.476669	50.866049
3470.366228	363603.844216	50.871053
3469.846174	363390.780655	50.876058
3468.652165	363174.947456	50.881063
3468.614718	362965.367849	50.886068
3467.567022	362762.893393	50.891073
3466.893873	362551.198752	50.896077
3466.429664	362341.760151	50.901082
3465.707104	362131.852563	50.906087
3465.384472	361912.059021	50.911092
3464.559917	361703.590571	50.916097
3463.668727	361487.091031	50.921101
3463.328653	361264.752709	50.926106
3462.462673	361054.175982	50.931111
3461.757647	360841.053759	50.936116
3460.931736	360617.669621	50.941121
3460.292164	360409.980513	50.946125
3459.628533	360211.658420	50.951130
3458.712545	360001.288530	50.956135
3458.356995	359783.526061	50.961140
3457.682486	359573.981298	50.966145
3456.890866	359362.952808	50.971149
3456.461198	359153.545643	50.976154
3455.406270	358933.218050	50.981159
3454.937029	358716.995570	50.986164
3454.247448	358522.131426	50.991169
3453.815390	358290.531295	50.996173
3453.310946	358097.417481	51.001178
3452.673684	357869.919346	51.006183
3451.710659	357650.894722	51.011188
3451.309127	357434.172407	51.016193
3450.044551	357224.125614	51.021197
3449.598910	357013.134127	51.026202
3448.808496	356808.558192	51.031207
3448.317150	356600.676813	51.036212
3447.826702	356390.809494	51.041217
3446.764867	356169.732717	51.046221
3446.599333	355956.453075	51.051226
3445.558252	355761.277434	51.056231
3444.838674	355539.507582	51.061236
3444.426450	355327.689411	51.066241
3443.489626	355110.023792	51.071245
3442.784148	354901.558536	51.076250
3442.337674	354684.322549	51.081255
3441.365602	354482.921609	51.086260
3440.610372	354274.894310	51.091265
3439.980076	354056.488641	51.096269
3439.789369	353845.469161	51.101274
3438.725411	353651.663373	51.106279
3438.110181	353433.125457	51.111284
3437.520510	353213.666404	51.116289
3436.734042	353015.844260	51.121293
3436.104118	352800.690825	51.126298
3435.209325	352586.850883	51.131303
3434.772045	352384.084791	51.136308
3434.065788	352174.997954	51.141313
3433.491381	351972.760973	51.146317
3432.761866	351758.611606	51.151322
3431.917994	351555.219490	51.156327
3431.691914	351343.024880	51.161332
3430.651200	351137.422668	51.166337
3430.070082	350922.075774	51.171341
3429.507666	350718.712341	51.176346
3428.885592	350513.779629	51.181351
3428.534882	350292.641921	51.186356
3427.580181	350082.110079	51.191361
3426.773332	349867.405519	51.196365
3426.212244	349642.531682	51.201370
3425.306991	349439.624909	51.206375
3424.591246	349227.372216	51.211380
3423.866310	349027.794998	51.216385
3423.492734	348822.434900	51.221389
3422.759966	348611.429666	51.226394
3422.229001	348397.006638	51.231399
3421.554221	348192.633561	51.236404
3420.506461	347986.511626	51.241409
3419.907322	347777.772794	51.246413
3419.732940	347560.363199	51.251418
3418.871382	347362.506938	51.256423
3418.064622	347145.246648	51.261428
3417.601207	346934.956105	51.266433
3416.565628	346731.220201	51.271437
3415.902425	346517.549076	51.276442
3415.059208	346314.621208	51.281447
3414.732670	346099.139054	51.286452
3413.904235	345905.319507	51.291457
3413.109336	345693.447851	51.296461
3412.959789	345483.153277	51.301466
3412.053834	345285.882301	51.306471
3411.647118	345069.085437	51.311476
3410.753280	344862.291601	51.316481
3410.052733	344649.204928	51.321485
3409.316800	344439.355677	51.326490
3408.615640	344237.288987	51.331495
3408.242899	344025.090011	51.336500
3407.237181	343815.917555	51.341505
3406.509020	343608.176801	51.346509
3406.118554	343407.101771	51.351514
3405.152531	343207.720685	51.356519
3404.489544	342988.793152	51.361524
3403.583169	342805.488316	51.366529
3402.900265	342587.784282	51.371533
3402.435423	342386.692159	51.376538
3401.911102	342191.336035	51.381543
3401.444344	341984.337450	51.386548
3400.507740	341783.267033	51.391553
3399.902684	341581.150794	51.396557
3399.297177	341365.237456	51.401562
3398.257839	341168.712236	51.406567
3397.474814	340955.396485	51.411572
3397.151944	340757.127546	51.416577
3396.695290	340561.933751	51.421581
3396.166699	340349.161162	51.426586
3395.091254	340136.856158	51.431591
3394.431727	339930.415776	51.436596
3393.781676	339727.256979	51.441601
3392.994488	339529.744895	51.446605
3392.709764	339319.043086	51.451610
3391.543466	339124.797109	51.456615
3390.900899	338921.660016	51.461620
3390.401460	338717.659601	51.466625
3389.730428	338511.063712	51.471629
3388.993233	338315.932845	51.476634
3388.313263	338121.632392	51.481639
3388.031920	337912.758290	51.486644
3387.164924	337715.329634	51.491649
3386.370175	337519.900008	51.496653
3385.748606	337305.146441	51.501658
3384.728629	337107.180107	51.506663
3384.480733	336903.057873	51.511668
3383.721848	336703.063428	51.516673
3383.207322	336501.196854	51.521677
3382.467437	336288.800727	51.526682
3381.418723	336087.195577	51.531687
3380.986779	335898.118946	51.536692
3380.414491	335692.491442	51.541697
3379.920374	335501.285139	51.546701
3379.300339	335294.340208	51.551706
3378.272455	335090.183074	51.556711
3377.781552	334890.344533	51.561716
3376.816576	334690.376720	51.566721
3376.235817	334482.506657	51.571725
3375.669460	334286.191428	51.576730
3374.809431	334098.501311	51.581735
3374.301374	333889.421462	51.586740
3373.686677	333692.068434	51.591745
3372.993986	333494.523521	51.596749
3372.437522	333298.356695	51.601754
3371.663332	333096.495705	51.606759
3371.130558	332896.556231	51.611764
3370.184264	332698.590952	51.616769
3369.627135	332497.788631	51.621773
3368.866282	332302.822455	51.626778
3368.110267	332106.200190	51.631783
3367.871114	331898.981317	51.636788
3367.042991	331707.741097	51.641793
3366.401458	331510.819062	51.646797
3365.768194	331299.485598	51.651802
3365.020537	331099.676950	51.656807
3364.256636	330908.118970	51.661812
3363.791209	330710.708672	51.666817
3362.925907	330511.629879	51.671821
3362.440611	330306.558510	51.676826
3361.469246	330103.880221	51.681831
3360.882061	329915.321353	51.686836
3360.386384	329715.290905	51.691841
3359.476643	329528.182330	51.696845
3359.068626	329327.551426	51.701850
3357.990082	329129.291919	51.706855
3357.593829	328927.843396	51.711860
3356.793358	328735.114503	51.716865
3356.159456	328538.056114	51.721869
3355.513463	328337.918513	51.726874
3354.575468	328147.093908	51.731879
3354.216041	327960.378193	51.736884
3353.802028	327762.570175	51.741889
3352.803059	327563.428413	51.746893
3352.196842	327368.526762	51.751898
3351.546751	327166.451839	51.756903
3351.232826	326973.132424	51.761908
3350.123179	326781.822435	51.766913
3349.712136	326585.207614	51.771917
3349.074446	326378.214899	51.776922
3347.871107	326187.885792	51.781927
3347.703530	325986.877278	51.786932
3347.095546	325801.621562	51.791937
3346.237496	325604.973197	51.796941
3345.693620	325397.504838	51.801946
3344.762721	325200.459648	51.806951
3344.221748	325008.749986	51.811956
3343.362859	324814.034865	51.816961
3342.716174	324613.175124	51.821965
3342.621699	324422.284613	51.826970
3341.685686	324237.433700	51.831975
3340.817950	324019.013970	51.836980
3340.126438	323825.670421	51.841985
3339.327492	323642.782483	51.846989
3339.018122	323444.514548	51.851994
3337.951100	323247.970037	51.856999
3337.497155	323062.301931	51.862004
3336.623647	322881.002749	51.867009
3335.924313	322675.003529	51.872013
3335.563340	322483.183267	51.877018
3334.775378	322289.367729	51.882023
3334.142274	322107.035903	51.887028
3333.705778	321899.363732	51.892033
3332.970675	321699.122191	51.897037
3332.397332	321513.749738	51.902042
3331.540397	321321.878065	51.907047
3331.199151	321119.077662	51.912052
3330.347276	320929.623221	51.917057
3329.464986	320737.168678	51.922061
3329.067628	320530.021818	51.927066
3328.181116	320350.272671	51.932071
3327.688174	320136.901820	51.937076
3326.682658	319948.029790	51.942081
3325.971290	319762.879260	51.947085
3325.625296	319564.786645	51.952090
3325.026527	319380.865191	51.957095
3324.363259	319178.238706	51.962100
3323.748862	318985.279787	51.967105
3322.742736	318791.720403	51.972109
3322.329971	318589.078485	51.977114
3321.254535	318397.337096	51.982119
3320.825006	318217.587927	51.987124
3320.220400	318009.195087	51.992129
3319.357102	317821.442097	51.997133
3318.682464	317635.466761	52.002138
3317.737302	317448.413489	52.007143
3317.751928	317258.432591	52.012148
3316.809042	317070.461567	52.017153
3315.782879	316873.998704	52.022157
3315.545001	316684.591355	52.027162
3314.947870	316509.601663	52.032167
3314.299357	316309.258479	52.037172
3313.666689	316117.009689	52.042177
3312.880629	315924.326453	52.047181
3312.363607	315722.382576	52.052186
3311.422989	315537.336579	52.057191
3310.910863	315339.312523	52.062196
3310.155282	315155.229638	52.067201
3309.210740	314977.414870	52.072205
3308.937767	314766.951156	52.077210
3308.215150	314591.468732	52.082215
3307.305942	314385.942964	52.087220
3306.791752	314211.216307	52.092225
3306.013837	314027.033102	52.097229
3305.693854	313821.107466	52.102234
3304.604527	313639.952107	52.107239
3304.277149	313441.462344	52.112244
3303.621398	313251.554566	52.117249
3302.706094	313064.132048	52.122253
3302.374344	312873.535759	52.127258
3301.354934	312685.288743	52.132263
3300.830658	312499.458566	52.137268
3300.068159	312295.127864	52.142273
3299.484779	312117.684095	52.147277
3298.554064	311916.536861	52.152282
3298.019658	311742.929847	52.157287
3297.308267	311538.589674	52.162292
3296.951511	311357.594780	52.167297
3295.916915	311176.070205	52.172301
3295.653837	310972.702141	52.177306
3294.812606	310782.004621	52.182311
3293.865845	310594.532008	52.187316
3293.637823	310413.566191	52.192321
3292.754540	310221.168275	52.197325
3292.038962	310028.259687	52.202330
3291.128948	309846.178567	52.207335
3290.818799	309658.782012	52.212340
3290.127800	309470.808786	52.217345
3289.312503	309294.365018	52.222349
3288.820840	309090.673347	52.227354
3288.086270	308919.029117	52.232359
3287.245423	308722.802342	52.237364
3286.684148	308527.702419	52.242369
3285.925767	308350.000497	52.247373
3285.568444	308157.974459	52.252378
3284.593334	307973.303394	52.257383
3284.204534	307794.370825	52.262388
3283.437202	307601.313789	52.267393
3282.684182	307407.974078	52.272397
3282.240181	307232.156201	52.277402
3281.548161	307033.229389	52.282407
3280.858399	306856.685916	52.287412
3280.016119	306668.375876	52.292417
3279.545253	306475.397581	52.297421
3279.053920	306280.716058	52.302426
3278.000980	306102.064455	52.307431
3277.636950	305900.741220	52.312436
3277.022958	305713.870707	52.317441
3276.162706	305531.444431	52.322445
3275.601471	305341.407329	52.327450
3274.935549	305150.189637	52.332455
3273.911757	304972.728814	52.337460
3273.345101	304787.148291	52.342465
3272.937617	304603.248546	52.347469
3272.294388	304405.354215	52.352474
3271.194139	304228.643046	52.357479
3270.604142	304036.927966	52.362484
3270.139878	303850.998956	52.367489
3268.986162	303670.399276	52.372493
3268.792508	303490.309614	52.377498
3267.695199	303307.306761	52.382503
3267.297289	303117.113497	52.387508
3266.620706	302940.868519	52.392513
3266.097818	302751.942390	52.397517
3265.450793	302564.894683	52.402522
3264.661324	302392.996149	52.407527
3264.116337	302197.935485	52.412532
3263.770957	302021.280509	52.417537
3262.591096	301830.063334	52.422541
3262.095279	301650.477649	52.427546
3261.563942	301472.501751	52.432551
3260.575483	301278.172201	52.437556
3259.952292	301099.726552	52.442561
3259.359688	300912.057042	52.447565
3258.690754	300713.601638	52.452570
3257.934691	300551.551283	52.457575
3257.407057	300357.300514	52.462580
3257.123583	300176.839185	52.467585
3256.312007	299987.573391	52.472589
3255.383428	299802.604268	52.477594
3254.814222	299616.635827	52.482599
3254.103628	299429.136086	52.487604
3253.732690	299242.193605	52.492609
3252.981427	299063.485878	52.497613
3252.447755	298869.616342	52.502618
3251.572920	298695.104316	52.507623
3250.983402	298503.458810	52.512628
3250.126842	298323.289912	52.517633
3249.521852	298123.649884	52.522637
3249.051701	297936.721705	52.527642
3248.021603	297759.100907	52.532647
3247.193380	297562.449727	52.537652
3246.923480	297377.195576	52.542657
3246.000765	297206.102246	52.547661
3245.700657	297015.046059	52.552666
3244.658061	296829.990006	52.557671
3244.104572	296648.600043	52.562676
3243.547930	296456.896271	52.567681
3242.940829	296276.864191	52.572685
3242.360575	296100.189349	52.577690
3241.426786	295916.999772	52.582695
3240.586764	295727.606687	52.587700
3240.024943	295552.583804	52.592705
3238.895144	295370.163284	52.597709
3238.690186	295197.248346	52.602714
3237.786014	295012.627105	52.607719
3237.425110	294837.622761	52.612724
3236.227061	294656.129228	52.617729
3235.671921	294471.019350	52.622733
3235.188108	294297.969516	52.627738
3234.431334	294118.366697	52.632743
3234.015191	293937.767551	52.637748
3233.318974	293765.795057	52.642753
3232.515670	293590.044736	52.647757
3232.425338	293398.824654	52.652762
3231.348998	293229.229417	52.657767
3231.077361	293045.423267	52.662772
3230.575031	292858.953918	52.667777
3229.730627	292675.696502	52.672781
3228.911787	292492.078356	52.677786
3228.391901	292315.874749	52.682791
3227.695891	292122.890316	52.687796
3226.954003	291938.419146	52.692801
3226.156326	291752.326741	52.697805
3225.494295	291572.656032	52.702810
3225.163897	291378.543541	52.707815
3224.291248	291200.408478	52.712820
3223.346696	291013.625674	52.717825
3222.569183	290842.300639	52.722829
3222.229892	290640.294032	52.727834
3221.396194	290473.612763	52.732839
3220.760027	290281.839927	52.737844
3220.329064	290097.369194	52.742849
3219.410627	289931.439565	52.747853
3218.805544	289741.011227	52.752858
3218.166827	289568.848469	52.757863
3217.257198	289387.712875	52.762868
3216.753498	289212.854427	52.767873
3215.972322	289032.054841	52.772877
3215.477094	288849.401689	52.777882
3214.620854	288677.960458	52.782887
3213.953536	288495.716338	52.787892
3213.645314	288309.569652	52.792897
3212.740104	288138.772567	52.797901
3212.143736	287947.144725	52.802906
3211.419195	287776.166058	52.807911
3210.770423	287592.263076	52.812916
3210.054953	287417.615408	52.817921
3209.303836	287241.648956	52.822925
3208.832887	287058.099570	52.827930
3208.107455	286889.132566	52.832935
3207.412462	286701.721840	52.837940
3206.740894	286531.014321	52.842945
3205.488931	286354.973863	52.847949
3204.968603	286172.068538	52.852954
3204.493808	286012.611986	52.857959
3203.954991	285825.660003	52.862964
3203.302919	285665.059825	52.867969
3202.654368	285478.379719	52.872973
3201.902844	285297.446137	52.877978
3201.149506	285140.019815	52.882983
3200.617985	284960.273748	52.887988
3200.311714	284772.494977	52.892993
3199.337677	284612.454695	52.897997
3198.974805	284426.187351	52.903002
3198.012709	284248.699375	52.908007
3197.479892	284058.995102	52.913012
3196.567510	283899.887136	52.918017
3195.277364	283718.987194	52.923021
3195.609843	283539.256674	52.928026
3194.744009	283380.064770	52.933031
3193.586915	283203.829738	52.938036
3193.391148	283019.674742	52.943041
3192.323167	282856.821772	52.948045
3192.161576	282665.530147	52.953050
3191.234841	282516.916936	52.958055
3190.311347	282336.366001	52.963060
3190.192586	282157.521399	52.968065
3189.218161	281982.479556	52.973069
3188.742947	281808.046322	52.978074
3188.035808	281642.996589	52.983079
3187.164641	281461.163706	52.988084
3186.940051	281281.724363	52.993089
3185.954160	281113.407728	52.998093
3185.221746	280945.814997	53.003098
3184.339942	280768.185886	53.008103
3183.804273	280600.511011	53.013108
3183.443037	280426.314082	53.018113
3182.622534	280258.302177	53.023117
3182.155239	280079.461253	53.028122
3181.582010	279912.759977	53.033127
3180.765197	279739.806533	53.038132
3180.013379	279558.285412	53.043137
3179.121977	279382.058290	53.048141
3178.558410	279217.087212	53.053146
3178.191799	279042.890870	53.058151
3177.259859	278870.897824	53.063156
3177.012213	278688.711009	53.068161
3176.136431	278527.201992	53.073165
3175.614072	278348.853381	53.078170
3174.750502	278173.258383	53.083175
3173.820112	277995.814745	53.088180
3173.423965	277816.732985	53.093185
3172.627143	277650.041297	53.098189
3171.882174	277475.828218	53.103194
3171.666018	277305.046086	53.108199
3170.655845	277126.570784	53.113204
3170.002531	276957.462304	53.118209
3169.125705	276788.185433	53.123213
3168.827182	276609.572023	53.128218
3168.129717	276440.113942	53.133223
3167.284054	276271.417886	53.138228
3167.027558	276095.140893	53.143233
3166.201044	275921.959360	53.148237
3165.429933	275747.190015	53.153242
3164.615082	275573.955692	53.158247
3164.134424	275411.085061	53.163252
3163.784195	275237.293319	53.168257
3162.717970	275055.847012	53.173261
3162.078403	274889.868916	53.178266
3161.381341	274711.063852	53.183271
3160.459723	274547.524422	53.188276
3160.312898	274367.282479	53.193281
3159.590428	274193.677005	53.198285
3158.818756	274016.055320	53.203290
3158.248258	273847.290280	53.208295
3157.185087	273675.750749	53.213300
3156.950885	273502.195399	53.218305
3155.903264	273334.142602	53.223309
3155.240413	273155.103001	53.228314
3154.718789	272986.483104	53.233319
3153.983449	272828.033454	53.238324
3153.306780	272651.721208	53.243329
3152.768886	272487.026067	53.248333
3151.830820	272308.284794	53.253338
3151.213624	272141.819458	53.258343
3150.250145	271978.974508	53.263348
3149.799937	271808.407856	53.268353
3149.019529	271643.496517	53.273357
3148.918315	271470.862692	53.278362
3148.286348	271312.345938	53.283367
3147.173632	271146.876020	53.288372
3146.541914	270965.998082	53.293377
3145.729613	270803.562356	53.298381
3145.063177	270635.704293	53.303386
3144.082138	270463.719241	53.308391
3143.909497	270304.416866	53.313396
3143.242481	270145.625714	53.318401
3142.586527	269978.250025	53.323405
3141.973496	269806.181414	53.328410
3141.248457	269644.190543	53.333415
3140.689894	269487.649047	53.338420
3139.751935	269317.694902	53.343425
3139.372381	269154.528872	53.348429
3138.681243	268982.676571	53.353434
3138.081864	268817.609823	53.358439
3137.391017	268655.384568	53.363444
3136.649703	268484.788290	53.368449
3135.675597	268315.604183	53.373453
3135.314302	268137.995042	53.378458
3134.855921	267981.794626	53.383463
3134.026630	267827.002765	53.388468
3133.239779	267650.021422	53.393473
3132.404399	267492.530991	53.398477
3131.938741	267323.495947	53.403482
3131.094902	267151.184472	53.408487
3130.293352	267003.417686	53.413492
3130.156164	266825.009481	53.418497
3129.022006	266674.060972	53.423501
3128.386598	266494.534728	53.428506
3127.895443	266332.737020	53.433511
3126.976395	266169.478994	53.438516
3126.753926	266014.719022	53.443521
3126.101180	265846.401755	53.448525
3125.627736	265677.266669	53.453530
3124.725550	265519.278118	53.458535
3123.944399	265348.842050	53.463540
3123.329298	265184.466645	53.468545
3122.754624	265015.398787	53.473549
3122.081308	264847.492674	53.478554
3121.338161	264679.826896	53.483559
3120.229953	264517.338036	53.488564
3120.137947	264359.731101	53.493569
3119.204404	264200.933068	53.498573
3118.616708	264026.493963	53.503578
3118.147475	263869.252550	53.508583
3117.097073	263707.824559	53.513588
3116.668889	263533.640601	53.518593
3115.824152	263387.995813	53.523597
3115.296502	263207.435306	53.528602
3114.774383	263041.747287	53.533607
3113.755335	262876.214393	53.538612
3113.260168	262723.740113	53.543617
3112.804965	262566.013196	53.548621
3112.014617	262388.270713	53.553626
3111.324574	262220.674131	53.558631
3110.108310	262059.935362	53.563636
3110.068942	261900.513032	53.568641
3109.085687	261740.501592	53.573645
3108.368429	261577.723088	53.578650
3107.843951	261420.058658	53.583655
3107.052352	261270.025983	53.588660
3106.529416	261107.522602	53.593665
3105.568021	260953.391186	53.598669
3105.309106	260789.216267	53.603674
3104.687165	260629.708553	53.608679
3103.751918	260473.051960	53.613684
3103.333530	260309.870335	53.618689
3102.348706	260153.578320	53.623693
3102.229881	259990.782431	53.628698
3101.532191	259818.527885	53.633703
3100.343236	259661.173357	53.638708
3100.028933	259504.291726	53.643713
3099.247003	259349.114123	53.648717
3098.516598	259183.104739	53.653722
3097.993735	259016.782476	53.658727
3097.500808	258862.909215	53.663732
3097.131352	258701.019706	53.668737
3095.816338	258541.852165	53.673741
3095.074062	258375.641462	53.678746
3094.926175	258212.291034	53.683751
3093.776564	258053.224979	53.688756
3093.621030	257886.386943	53.693761
3092.717696	257738.054854	53.698765
3092.242769	257563.856576	53.703770
3091.410983	257400.742285	53.708775
3090.720320	257246.213749	53.713780
3090.089302	257067.914841	53.718785
3089.038032	256916.346881	53.723789
3088.432448	256759.207549	53.728794
3087.737835	256599.382887	53.733799
3087.140674	256443.312076	53.738804
3086.554029	256283.878036	53.743809
3085.912299	256140.064251	53.748813
3085.217482	255973.032858	53.753818
3084.580477	255818.929787	53.758823
3083.745204	255660.554254	53.763828
3083.679839	255491.564521	53.768833
3082.601186	255342.625134	53.773837
3082.181588	255177.639131	53.778842
3081.753087	255023.630993	53.783847
3080.596922	254854.585222	53.788852
3080.090451	254682.406190	53.793857
3079.359573	254538.658575	53.798861
3078.567680	254376.176993	53.803866
3078.081704	254216.932374	53.808871
3077.372770	254061.314017	53.813876
3077.021602	253896.954931	53.818881
3076.155426	253737.745416	53.823885
3075.285351	253573.774340	53.828890
3074.682054	253421.450489	53.833895
3073.788316	253267.593784	53.838900
3073.658018	253098.387203	53.843905
3072.710191	252953.630987	53.848909
3072.318422	252783.600207	53.853914
3071.438587	252627.551696	53.858919
3070.873136	252460.630190	53.863924
3070.384735	252288.781565	53.868929
3069.398666	252139.193380	53.873933
3068.565833	251974.148255	53.878938
3068.182641	251822.554921	53.883943
3067.515465	251649.614686	53.888948
3066.844426	251484.417086	53.893953
3066.119840	251330.637156	53.898957
3065.323560	251173.685391	53.903962
3064.948459	251006.709691	53.908967
3063.816759	250866.797487	53.913972
3063.459049	250686.041966	53.918977
3063.089871	250536.484885	53.923981
3062.081978	250380.484153	53.928986
3061.624049	250217.800722	53.933991
3060.751650	250060.658329	53.938996
3060.336513	249892.187580	53.944001
3059.686661	249730.757402	53.949005
3058.959676	249583.193275	53.954010
3058.259236	249416.143367	53.959015
3057.314994	249258.605677	53.964020
3057.171446	249094.447522	53.969025
3056.130808	248930.355130	53.974029
3055.236056	248781.392206	53.979034
3054.692933	248620.964930	53.984039
3053.765516	248456.193005	53.989044
3053.343878	248303.895999	53.994049
3052.755524	248162.397689	53.999053
3052.017189	248003.835523	54.004058
3051.620573	247839.387716	54.009063
3050.872809	247690.097014	54.014068
3050.303049	247519.819786	54.019073
3049.493723	247355.794366	54.024077
3048.690653	247208.677513	54.029082
3048.022968	247046.107047	54.034087
3047.315646	246897.752993	54.039092
3047.104276	246732.131151	54.044097
3046.039641	246585.692982	54.049101
3045.318681	246419.082598	54.054106
3044.481631	246266.344156	54.059111
3044.310260	246130.562555	54.064116
3043.564518	245960.697024	54.069121
3042.896419	245808.849106	54.074125
3042.258473	245650.884828	54.079130
3041.491754	245486.447383	54.084135
3040.743035	245339.960524	54.089140
3040.432101	245168.219094	54.094145
3039.406679	245022.744065	54.099149
3038.989630	244860.442068	54.104154
3038.414202	244705.754045	54.109159
3037.625141	244543.180266	54.114164
3037.018502	244395.602401	54.119169
3036.055446	244228.523707	54.124173
3035.615758	244062.864841	54.129178
3034.643249	243915.778338	54.134183
3034.101073	243749.677718	54.139188
3033.632956	243606.382452	54.144193
3032.960726	243448.324360	54.149197
3032.235862	243297.175861	54.154202
3031.808294	243129.504526	54.159207
3031.335920	242983.256676	54.164212
3030.585836	242813.192158	54.169217
3029.831312	242663.678878	54.174221
3028.983531	242494.088630	54.179226
3027.982843	242335.778344	54.184231
3027.391429	242184.049834	54.189236
3027.039886	242021.155367	54.194241
3026.117186	241864.641354	54.199245
3025.653967	241707.698303	54.204250
3025.404519	241550.874407	54.209255
3024.467045	241396.044016	54.214260
3023.518316	241234.416514	54.219265
3022.958061	241076.954885	54.224269
3022.288227	240921.013226	54.229274
3021.986357	240765.140851	54.234279
3020.938567	240613.613883	54.239284
3020.370135	240437.794401	54.244289
3019.716535	240286.791144	54.249293
3018.635176	240139.064325	54.254298
3018.520202	239979.445592	54.259303
3017.639040	239827.282124	54.264308
3017.019383	239660.664600	54.269313
3016.094354	239517.217322	54.274317
3015.628584	239361.067206	54.279322
3015.187294	239209.267829	54.284327
3014.127281	239059.400024	54.289332
3013.659304	238891.537335	54.294337
3013.274993	238731.275453	54.299341
3012.113663	238577.350058	54.304346
3011.539100	238413.400980	54.309351
3010.752019	238266.317559	54.314356
3009.960845	238110.373486	54.319361
3009.230644	237965.649623	54.324365
3008.524112	237808.928661	54.329370
3008.212154	237662.127339	54.334375
3006.927340	237515.811247	54.339380
3006.637617	237356.045681	54.344385
3006.091234	237215.367947	54.349389
3005.404884	237068.906802	54.354394
3004.846934	236915.626701	54.359399
3003.995419	236760.763611	54.364404
3003.498224	236613.381921	54.369409
3002.629407	236464.658761	54.374413
3001.783989	236311.883389	54.379418
3001.199120	236160.492957	54.384423
3000.728163	236027.367559	54.389428
3000.151761	235876.969279	54.394433
2999.576498	235731.129005	54.399437
2998.635948	235577.504016	54.404442
2998.156649	235418.739019	54.409447
2997.243650	235284.284068	54.414452
2996.932291	235137.257011	54.419457
2996.245138	234990.213266	54.424461
2995.359519	234837.522840	54.429466
2995.064692	234686.801646	54.434471
2994.203702	234540.753679	54.439476
2993.802757	234378.183896	54.444481
2993.110940	234231.956822	54.449485
2992.111779	234080.584147	54.454490
2991.655514	233929.023910	54.459495
2991.047666	233776.749475	54.464500
2990.477452	233618.307281	54.469505
2989.580043	233470.993512	54.474509
2988.967699	233316.759860	54.479514
2988.587778	233164.424836	54.484519
2987.664761	233015.129711	54.489524
2986.817423	232857.267349	54.494529
2986.205148	232706.090193	54.499533
2985.573058	232563.599190	54.504538
2985.094216	232409.880574	54.509543
2984.302845	232265.174519	54.514548
2983.407218	232114.603337	54.519553
2982.897666	231965.371717	54.524557
2982.451378	231812.565570	54.529562
2981.817404	231655.384381	54.534567
2980.660804	231520.489408	54.539572
2980.250079	231367.169111	54.544577
2979.650122	231217.469213	54.549581
2979.331591	231057.540092	54.554586
2978.408051	230907.891922	54.559591
2977.410429	230766.301777	54.564596
2976.727547	230612.338342	54.569601
2976.317124	230465.486888	54.574605
2975.378685	230316.478599	54.579610
2974.848476	230166.591143	54.584615
2974.174236	230027.802703	54.589620
2973.830092	229875.951163	54.594625
2973.316083	229724.126772	54.599629
2972.259115	229572.719598	54.604634
2971.744880	229415.599700	54.609639
2970.966939	229268.884769	54.614644
2970.296495	229126.888946	54.619649
2969.492267	228992.400269	54.624653
2969.094236	228838.114710	54.629658
2968.726654	228677.866587	54.634663
2967.573533	228538.519751	54.639668
2966.817495	228371.840989	54.644673
2966.318908	228231.219795	54.649677
2965.874822	228083.970229	54.654682
2965.000898	227930.856461	54.659687
2964.352048	227786.949800	54.664692
2963.868826	227638.128589	54.669697
2963.156816	227481.349025	54.674701
2962.221377	227336.113586	54.679706
2961.758566	227183.368913	54.684711
2960.872774	227046.400989	54.689716
2960.296231	226889.626533	54.694721
2959.909659	226753.178387	54.699725
2959.123123	226600.778821	54.704730
2958.508962	226453.317126	54.709735
2957.712619	226307.004814	54.714740
2957.072930	226148.026647	54.719745
2956.210658	226004.971564	54.724749
2955.353901	225861.101110	54.729754
2954.957326	225713.478980	54.734759
2953.953943	225574.011486	54.739764
2953.689927	225429.513273	54.744769
2952.733941	225284.144634	54.749773
2952.092712	225141.348859	54.754778
2951.680163	224998.491669	54.759783
2950.634191	224858.955761	54.764788
2950.221528	224715.653531	54.769793
2949.995292	224577.312271	54.774797
2948.924102	224433.962039	54.779802
2948.227731	224290.654563	54.784807
2947.403276	224145.623598	54.789812
2946.865783	223991.916466	54.794817
2946.385011	223853.935009	54.799821
2945.613797	223712.346253	54.804826
2944.716302	223566.309508	54.809831
2943.959922	223427.990529	54.814836
2943.542689	223281.610947	54.819841
2942.938705	223137.056127	54.824845
2942.093880	223004.747704	54.829850
2941.813479	222856.259547	54.834855
2940.859117	222713.594093	54.839860
2940.278965	222568.094546	54.844865
2939.692095	222429.012173	54.849869
2939.085916	222286.559708	54.854874
2938.593702	222130.825029	54.859879
2937.652336	221991.099435	54.864884
2937.413736	221846.438262	54.869889
2936.801402	221702.663966	54.874893
2935.833519	221546.662086	54.879898
2935.174133	221402.030191	54.884903
2934.509501	221264.095191	54.889908
2933.837051	221107.894687	54.894913
2933.627086	220962.530540	54.899917
2932.653109	220810.782831	54.904922
2931.823469	220659.343546	54.909927
2930.896301	220525.168497	54.914932
2930.532862	220382.070172	54.919937
2929.769149	220239.315545	54.924941
2929.057987	220096.005507	54.929946
2928.583331	219936.326466	54.934951
2927.870740	219795.193969	54.939956
2927.113292	219654.896254	54.944961
2926.654672	219511.089115	54.949965
2925.757357	219366.880733	54.954970
2925.235828	219212.989798	54.959975
2924.508585	219072.128334	54.964980
2923.683837	218927.794771	54.969985
2923.137411	218780.897046	54.974989
2922.488076	218646.872390	54.979994
2922.112793	218504.823409	54.984999
2921.124365	218362.566290	54.990004
2920.260828	218209.279001	54.995009
2919.489778	218062.685623	55.000013
2919.185221	217931.446304	55.005018
2918.574331	217785.006347	55.010023
2917.777810	217645.024233	55.015028
2917.488609	217499.310403	55.020033
2916.642014	217340.472474	55.025037
2915.748664	217206.056386	55.030042
2915.498541	217060.744602	55.035047
2914.573442	216920.491525	55.040052
2913.716650	216768.351897	55.045057
2913.107088	216632.491807	55.050061
2912.368342	216490.351682	55.055066
2911.890882	216335.034388	55.060071
2910.966195	216209.255294	55.065076
2910.471194	216072.996301	55.070081
2909.795707	215927.257820	55.075085
2908.918662	215787.037619	55.080090
2908.590694	215643.637706	55.085095
2907.797651	215505.390450	55.090100
2907.032804	215355.797838	55.095105
2906.531224	215229.533508	55.100109
2905.622485	215087.181368	55.105114
2905.117122	214938.426860	55.110119
2904.098838	214807.115544	55.115124
2903.900720	214660.845968	55.120129
2903.011715	214526.892668	55.125133
2902.262787	214386.476883	55.130138
2902.137235	214248.202883	55.135143
2900.897385	214110.742024	55.140148
2900.149598	213969.245027	55.145153
2899.830994	213832.402573	55.150157
2898.975084	213696.027327	55.155162
2898.291625	213554.317379	55.160167
2897.601640	213428.773606	55.165172
2897.122212	213273.400032	55.170177
2896.486944	213133.338023	55.175181
2895.539203	213005.659357	55.180186
2895.155645	212866.258112	55.185191
2894.370275	212729.695510	55.190196
2893.818633	212590.919688	55.195201
2893.047158	212448.373290	55.200205
2892.335613	212318.532992	55.205210
2891.778799	212179.453397	55.210215
2891.052433	212043.226555	55.215220
2890.374642	211900.526525	55.220225
2889.739914	211768.485968	55.225229
2888.728350	211635.970783	55.230234
2888.485525	211499.783079	55.235239
2887.783466	211360.002772	55.240244
2887.044684	211214.399260	55.245249
2886.333540	211089.652502	55.250253
2885.625661	210958.083406	55.255258
2885.134885	210811.830617	55.260263
2884.282412	210683.581464	55.265268
2883.687307	210548.635257	55.270273
2883.156922	210409.720800	55.275277
2882.344127	210277.826091	55.280282
2881.774196	210141.133093	55.285287
2880.960070	210010.015542	55.290292
2880.252761	209875.750384	55.295297
2879.790088	209732.741176	55.300301
2879.276380	209599.947800	55.305306
2878.468286	209453.442972	55.310311
2877.763544	209330.365998	55.315316
2876.844849	209195.906692	55.320321
2876.555248	209059.133504	55.325325
2875.857990	208930.379748	55.330330
2875.090300	208789.177395	55.335335
2874.675523	208656.421295	55.340340
2873.813096	208513.261855	55.345345
2873.403673	208383.063676	55.350349
2872.383605	208249.844313	55.355354
2871.889803	208097.603909	55.360359
2871.259674	207970.037902	55.365364
2870.536082	207837.956119	55.370369
2870.210238	207690.271897	55.375373
2868.965280	207566.685857	55.380378
2868.623654	207426.615548	55.385383
2867.671010	207289.136810	55.390388
2867.025926	207148.517036	55.395393
2866.323511	207022.644443	55.400397
2865.383544	206888.562707	55.405402
2865.438069	206752.860203	55.410407
2864.444165	206634.034365	55.415412
2863.809341	206494.203576	55.420417
2863.494418	206356.346017	55.425421
2862.242276	206214.271918	55.430426
2861.873428	206079.732499	55.435431
2861.286262	205946.106100	55.440436
2860.452934	205817.329664	55.445441
2860.100295	205682.699499	55.450445
2859.108995	205559.993796	55.455450
2858.754925	205414.368690	55.460455
2857.616029	205280.767549	55.465460
2856.830065	205144.858232	55.470465
2856.207344	205018.735503	55.475469
2855.417698	204889.674218	55.480474
2854.932542	204755.805318	55.485479
2854.179118	204628.940552	55.490484
2853.744291	204500.345731	55.495489
2853.261842	204365.522830	55.500493
2852.362983	204239.547345	55.505498
2851.868812	204104.306947	55.510503
2851.361880	203975.864709	55.515508
2850.804807	203845.636302	55.520513
2849.902464	203709.290664	55.525517
2849.178112	203568.526639	55.530522
2848.826513	203438.648410	55.535527
2847.896246	203305.756946	55.540532
2847.246537	203165.414790	55.545537
2846.879088	203037.614341	55.550541
2845.911750	202906.358623	55.555546
2845.577479	202765.293031	55.560551
2844.810955	202630.150183	55.565556
2843.962856	202490.693767	55.570561
2843.611499	202357.967385	55.575565
2842.725600	202227.514818	55.580570
2842.344477	202084.714917	55.585575
2841.097321	201961.752068	55.590580
2840.401412	201816.852046	55.595585
2840.060883	201676.515565	55.600589
2839.667725	201547.577281	55.605594
2838.952909	201408.764210	55.610599
2838.272034	201278.726807	55.615604
2837.317150	201144.380946	55.620609
2836.775197	201005.770577	55.625613
2836.229395	200878.639615	55.630618
2835.506194	200735.006591	55.635623
2834.455879	200607.345333	55.640628
2833.968402	200471.489123	55.645633
2833.412161	200329.472311	55.650637
2832.808643	200215.828260	55.655642
2832.244633	200077.440076	55.660647
2831.517653	199933.300754	55.665652
2830.958367	199800.931611	55.670657
2830.292425	199665.894652	55.675661
2829.154224	199531.645436	55.680666
2829.077093	199389.784272	55.685671
2827.922105	199267.194663	55.690676
2827.153088	199134.122317	55.695681
2826.547534	199000.413610	55.700685
2825.790276	198870.228659	55.705690
2825.586941	198741.534208	55.710695
2824.721699	198612.588594	55.715700
2823.934826	198482.778308	55.720705
2823.333904	198350.228475	55.725709
2822.861924	198211.028870	55.730714
2822.356560	198081.035012	55.735719
2821.551917	197960.619792	55.740724
2820.840742	197823.355095	55.745729
2820.373228	197678.659063	55.750733
2819.590383	197547.807008	55.755738
2818.975879	197411.418813	55.760743
2818.431080	197277.882990	55.765748
2817.744204	197140.819829	55.770753
2816.988404	197004.124234	55.775757
2816.015250	196875.149078	55.780762
2815.401698	196732.960093	55.785767
2814.848961	196604.580703	55.790772
2813.997477	196471.833546	55.795777
2813.700790	196336.670286	55.800781
2812.707411	196219.571895	55.805786
2811.937620	196082.181109	55.810791
2811.433131	195954.699129	55.815796
2810.658978	195823.302904	55.820801
2810.173133	195691.403281	55.825805
2809.147231	195559.055111	55.830810
2808.733977	195428.137164	55.835815
2808.186633	195309.188820	55.840820
2807.215849	195172.341280	55.845825
2806.807963	195036.435613	55.850829
2805.879653	194914.863736	55.855834
2805.201467	194786.686912	55.860839
2804.363983	194654.145846	55.865844
2804.281144	194531.639371	55.870849
2803.614491	194409.823685	55.875853
2802.501161	194275.253295	55.880858
2802.028453	194133.532756	55.885863
2801.509792	194020.066912	55.890868
2800.759661	193894.372189	55.895873
2800.662501	193749.692217	55.900877
2799.756802	193624.022813	55.905882
2799.130858	193483.817067	55.910887
2798.234767	193352.382970	55.915892
2797.666586	193209.293290	55.920897
2797.069510	193077.392681	55.925901
2796.154023	192953.431494	55.930906
2795.713893	192821.939311	55.935911
2794.865086	192695.372601	55.940916
2794.086814	192568.502403	55.945921
2793.576684	192429.629994	55.950925
2792.741101	192311.256098	55.955930
2791.960769	192168.724699	55.960935
2791.516436	192052.401546	55.965940
2791.085338	191924.803688	55.970945
2790.402276	191794.116135	55.975949
2789.499365	191659.952129	55.980954
2789.285755	191519.368590	55.985959
2788.603662	191385.348492	55.990964
2787.667560	191256.992638	55.995969
2787.117551	191126.565717	56.000973
2786.280165	190997.202513	56.005978
2785.844128	190859.569707	56.010983
2785.215897	190742.375482	56.015988
2784.219983	190601.893069	56.020993
2783.861085	190472.748115	56.025997
2783.080098	190339.446350	56.031002
2782.700700	190199.376384	56.036007
2781.953598	190064.886787	56.041012
2781.150064	189936.309897	56.046017
2780.584248	189794.782073	56.051021
2779.739503	189660.970667	56.056026
2779.392940	189525.693954	56.061031
2778.318813	189395.990895	56.066036
2777.654102	189265.816219	56.071041
2777.239324	189138.643017	56.076045
2776.366950	189013.514636	56.081050
2776.100632	188872.616425	56.086055
2775.285092	188737.848814	56.091060
2774.313359	188597.203105	56.096065
2773.697011	188464.605714	56.101069
2773.133068	188339.099493	56.106074
2772.460673	188203.063951	56.111079
2771.672406	188077.148681	56.116084
2770.897997	187944.030742	56.121089
2770.644889	187813.222396	56.126093
2769.868741	187692.776813	56.131098
2769.125827	187565.227301	56.136103
2768.855002	187431.814786	56.141108
2767.928202	187302.132360	56.146113
2767.462969	187163.726178	56.151117
2766.688127	187034.440261	56.156122
2765.732410	186887.181730	56.161127
2764.812506	186765.260139	56.166132
2764.056706	186632.842733	56.171137
2764.090367	186503.099477	56.176141
2762.703796	186375.120891	56.181146
2762.367005	186253.324570	56.186151
2761.847138	186123.161194	56.191156
2761.198514	185988.807686	56.196161
2760.605138	185859.738054	56.201165
2759.665318	185736.092210	56.206170
2759.516630	185600.019564	56.211175
2758.517415	185471.129815	56.216180
2757.838191	185341.184743	56.221185
2757.070685	185202.132692	56.226189
2756.414873	185076.204676	56.231194
2756.065656	184956.347467	56.236199
2755.225812	184807.856049	56.241204
2754.613697	184690.305603	56.246209
2754.211219	184547.762980	56.251213
2753.502231	184425.356299	56.256218
2752.709635	184289.898453	56.261223
2751.921792	184157.900438	56.266228
2751.364842	184026.972984	56.271233
2751.141790	183890.179457	56.276237
2749.950480	183762.330014	56.281242
2749.158383	183623.019616	56.286247
2748.726719	183497.785638	56.291252
2747.907432	183367.728548	56.296257
2747.450895	183231.940829	56.301261
2746.558127	183105.458020	56.306266
2746.145494	182972.081121	56.311271
2745.560278	182845.804758	56.316276
2744.660158	182710.432372	56.321281
2744.173028	182572.145530	56.326285
2743.408033	182431.931424	56.331290
2742.900580	182302.515004	56.336295
2742.082968	182169.980654	56.341300
2741.170513	182040.807252	56.346305
2740.632605	181908.051301	56.351309
2740.191125	181778.943997	56.356314
2739.479581	181646.127306	56.361319
2738.711408	181513.281830	56.366324
2737.781990	181389.799099	56.371329
2737.530435	181254.888192	56.376333
2736.708533	181133.297220	56.381338
2736.153863	180999.656278	56.386343
2735.481043	180867.726263	56.391348
2734.831497	180724.344752	56.396353
2734.178990	180597.360519	56.401357
2733.479031	180475.866568	56.406362
2733.061347	180340.196189	56.411367
2732.111822	180205.895216	56.416372
2731.262337	180076.030832	56.421377
2730.940136	179939.799635	56.426381
2730.064006	179814.608509	56.431386
2729.633675	179681.829655	56.436391
2729.007493	179540.063841	56.441396
2728.216248	179415.967072	56.446401
2727.553542	179280.059042	56.451405
2726.761101	179149.018230	56.456410
2726.580306	179003.418605	56.461415
2725.802040	178869.705272	56.466420
2724.732279	178746.010739	56.471425
2724.578368	178610.431292	56.476429
2723.601915	178480.070408	56.481434
2723.085671	178352.206369	56.486439
2722.509860	178214.990615	56.491444
2721.660119	178069.958089	56.496449
2721.165806	177931.432970	56.501453
2720.028136	177808.578722	56.506458
2719.688336	177672.128681	56.511463
2719.291540	177538.092059	56.516468
2718.491287	177407.070644	56.521473
2718.161327	177269.501071	56.526477
2716.989767	177136.020932	56.531482
2716.563045	176998.480304	56.536487
2716.069449	176863.914271	56.541492
2715.179030	176722.327040	56.546497
2714.260205	176590.589290	56.551501
2713.422769	176459.576767	56.556506
2713.136214	176319.536001	56.561511
2712.802378	176189.118663	56.566516
2711.727589	176055.677569	56.571521
2711.409032	175910.886427	56.576525
2710.250820	175768.556342	56.581530
2709.866714	175642.282296	56.586535
2709.375372	175504.973118	56.591540
2708.480659	175369.343568	56.596545
2708.133168	175239.592788	56.601549
2707.203384	175105.750273	56.606554
2706.439710	174972.047225	56.611559
2705.959640	174827.705227	56.616564
2705.280078	174697.487331	56.621569
2704.821762	174559.654664	56.626573
2703.940003	174415.097970	56.631578
2703.036895	174280.974156	56.636583
2702.438350	174140.150908	56.641588
2702.046829	174012.000819	56.646593
2701.360453	173873.977700	56.651597
2700.641668	173742.471855	56.656602
2700.087931	173597.039463	56.661607
2699.401041	173458.560008	56.666612
2698.693095	173327.562531	56.671617
2698.012175	173188.192810	56.676621
2697.213652	173044.747051	56.681626
2696.675921	172907.034390	56.686631
2695.813243	172774.371775	56.691636
2695.204208	172640.105139	56.696641
2694.910986	172503.983011	56.701645
2693.833789	172376.938785	56.706650
2693.285212	172233.761587	56.711655
2692.593115	172098.848631	56.716660
2691.881902	171965.973970	56.721665
2691.699869	171826.123046	56.726669
2690.669115	171690.133287	56.731674
2690.671531	171542.013251	56.736679
2689.835453	171411.703725	56.741684
2688.982159	171273.042091	56.746689
2688.337727	171127.327933	56.751693
2687.714395	170987.855126	56.756698
2687.130735	170845.896686	56.761703
2686.169898	170706.745416	56.766708
2685.403943	170574.202083	56.771713
2684.734810	170425.862029	56.776717
2684.261809	170296.007395	56.781722
2683.528780	170146.788342	56.786727
2682.784175	170018.249364	56.791732
2682.097298	169885.543257	56.796737
2681.514971	169740.358574	56.801741
2680.805558	169612.374912	56.806746
2680.067545	169470.115335	56.811751
2679.720207	169325.874173	56.816756
2679.057477	169186.045321	56.821761
2678.458259	169041.425485	56.826765
2677.487424	168915.024272	56.831770
2676.895275	168772.858622	56.836775
2676.190153	168635.912423	56.841780
2675.459843	168490.794067	56.846785
2675.199229	168356.080115	56.851789
2674.019443	168221.919188	56.856794
2673.612456	168080.413467	56.861799
2673.163844	167940.606124	56.866804
2672.090557	167809.812294	56.871809
2671.790680	167669.473740	56.876813
2670.879818	167536.200914	56.881818
2670.245039	167383.531034	56.886823
2669.664219	167251.186058	56.891828
2668.611813	167117.606523	56.896833
2668.264229	166970.665848	56.901837
2667.892510	166838.378208	56.906842
2667.270467	166700.879074	56.911847
2666.739963	166553.689265	56.916852
2665.610365	166404.980062	56.921857
2665.075824	166267.049042	56.926861
2664.548601	166142.456031	56.931866
2664.024998	165989.837792	56.936871
2663.190958	165842.953190	56.941876
2662.269450	165705.873921	56.946881
2661.752111	165561.941099	56.951885
2661.115415	165427.284522	56.956890
2660.834967	165286.989972	56.961895
2659.931090	165137.627032	56.966900
2659.171513	165005.076763	56.971905
2658.676750	164853.259696	56.976909
2657.571333	164715.615627	56.981914
2657.081606	164564.320274	56.986919
2657.014028	164428.992279	56.991924
2655.960775	164298.118610	56.996929
2655.614155	164151.036370	57.001933
2654.586647	163999.332673	57.006938
2653.848111	163853.737787	57.011943
2653.556129	163712.166882	57.016948
2652.641288	163567.605540	57.021953
2651.775085	163425.122270	57.026957
2650.950977	163295.881513	57.031962
2650.583725	163149.404169	57.036967
2650.175859	163009.367394	57.041972
2648.998074	162866.287247	57.046977
2649.117968	162724.921935	57.051981
2648.104991	162587.601838	57.056986
2647.314909	162436.273917	57.061991
2647.201375	162291.705137	57.066996
2645.891789	162142.380617	57.072001
2645.959356	161996.398480	57.077005
2645.040622	161854.069589	57.082010
2644.227026	161709.601358	57.087015
2643.591091	161550.776882	57.092020
2642.279498	161413.317883	57.097025
2642.138855	161266.634300	57.102029
2641.497993	161127.188474	57.107034
2640.913081	160989.374408	57.112039
2640.093161	160845.139528	57.117044
2639.571939	160694.729906	57.122049
2638.953601	160553.108722	57.127053
2638.254494	160408.030090	57.132058
2637.593046	160252.228577	57.137063
2636.767580	160112.676139	57.142068
2635.943608	159971.496698	57.147073
2635.478867	159821.933638	57.152077
2634.555372	159685.691190	57.157082
2634.076964	159543.072960	57.162087
2633.599657	159398.789702	57.167092
2632.882321	159255.714681	57.172097
2632.336040	159100.128858	57.177101
2631.154650	158972.168147	57.182106
2630.563799	158821.523298	57.187111
2630.342076	158686.915223	57.192116
2629.375349	158542.992729	57.197121
2629.138874	158391.301980	57.202125
2628.260476	158253.163754	57.207130
2627.757509	158112.741858	57.212135
2627.247443	157961.795536	57.217140
2626.377865	157814.072286	57.222145
2626.059258	157656.626219	57.227149
2624.951297	157514.535563	57.232154
2624.335092	157363.545107	57.237159
2623.824031	157216.009145	57.242164
2622.915820	157070.519876	57.247169
2622.471405	156922.173734	57.252173
2621.879371	156784.034149	57.257178
2621.134617	156621.893237	57.262183
2620.546156	156475.847336	57.267188
2619.923043	156343.498482	57.272193
2619.198414	156187.191299	57.277197
2618.322683	156043.875006	57.282202
2617.715620	155883.470036	57.287207
2617.247212	155743.967601	57.292212
2616.600583	155599.078741	57.297217
2615.759719	155450.534862	57.302221
2615.240749	155302.525367	57.307226
2614.702030	155158.778055	57.312231
2613.806726	155000.100874	57.317236
2613.181059	154852.275506	57.322241
2612.924601	154704.010937	57.327245
2611.655815	154561.665713	57.332250
2611.496059	154408.976250	57.337255
2610.723752	154249.253493	57.342260
2609.955044	154100.360920	57.347265
2609.327141	153951.573809	57.352269
2608.685619	153806.526595	57.357274
2608.083668	153650.351532	57.362279
2607.262552	153505.156130	57.367284
2606.407622	153354.869614	57.372289
2606.173449	153202.286421	57.377293
2605.285587	153052.464081	57.382298
2604.663448	152898.113396	57.387303
2604.151505	152742.042726	57.392308
2603.185920	152599.848484	57.397313
2602.784129	152446.507260	57.402317
2602.085532	152302.873817	57.407322
2601.104817	152154.214206	57.412327
2600.695459	151994.826070	57.417332
2599.756303	151848.932131	57.422337
2599.508532	151703.208906	57.427341
2599.073836	151557.185480	57.432346
2598.179779	151413.078479	57.437351
2597.440428	151251.127931	57.442356
2596.841408	151041.162611	57.447361
2596.220222	150881.686344	57.452365
2595.516798	150743.551217	57.457370
2594.978222	150589.096438	57.462375
2594.658009	150433.616419	57.467380
2593.601684	150276.321904	57.472385
2593.181704	150119.931379	57.477389
2592.365310	149963.362943	57.482394
2591.462232	149812.350389	57.487399
2591.300132	149656.391489	57.492404
2590.316300	149503.207133	57.497409
2589.408807	149343.262701	57.502413
2588.935302	149197.904187	57.507418
2588.399954	149042.363263	57.512423
2587.747437	148884.121880	57.517428
2586.920016	148742.443644	57.522433
2586.484130	148569.515789	57.527437
2585.798032	148417.738260	57.532442
2584.958062	148257.547059	57.537447
2584.616276	148119.785243	57.542452
2583.656359	147968.625141	57.547457
2583.234660	147807.391331	57.552461
2582.280181	147650.512908	57.557466
2581.793514	147485.719861	57.562471
2581.634415	147328.373847	57.567476
2580.323404	147177.298560	57.572481
2580.052203	147015.841576	57.577485
2578.865581	146859.677402	57.582490
2578.190664	146709.177094	57.587495
2578.169664	146557.239502	57.592500
2577.132244	146395.309821	57.597505
2576.484860	146240.029085	57.602509
2575.712227	146087.424963	57.607514
2575.088942	145931.938599	57.612519
2574.637455	145772.715043	57.617524
2573.577189	145622.293708	57.622529
2573.050053	145465.066142	57.627533
2572.575682	145314.248450	57.632538
2571.898045	145156.665050	57.637543
2571.546236	144997.239026	57.642548
2570.644918	144836.299741	57.647553
2570.212292	144676.062172	57.652557
2569.268144	144519.337516	57.657562
2568.460190	144359.631237	57.662567
2568.243509	144206.350953	57.667572
2567.131104	144058.054861	57.672577
2566.455571	143892.954813	57.677581
2565.642452	143736.098990	57.682586
2565.191656	143587.153900	57.687591
2564.601776	143426.820644	57.692596
2563.934648	143273.413061	57.697601
2563.284129	143117.995918	57.702605
2562.562337	142956.072243	57.707610
2561.891043	142806.492413	57.712615
2561.544676	142632.617398	57.717620
2560.678638	142487.796885	57.722625
2559.934707	142332.538302	57.727629
2559.353315	142170.024737	57.732634
2558.933669	142003.331393	57.737639
2558.144629	141844.486517	57.742644
2557.285371	141698.817349	57.747649
2556.959752	141538.579169	57.752653
2556.105974	141385.871368	57.757658
2555.425847	141215.322825	57.762663
2555.001879	141065.839404	57.767668
2554.014787	140909.305198	57.772673
2553.386488	140739.081482	57.777677
2552.768171	140592.528154	57.782682
2551.690595	140434.854517	57.787687
2551.576863	140270.803145	57.792692
2550.549158	140111.408027	57.797697
2550.121199	139952.985974	57.802701
2549.316618	139795.259723	57.807706
2548.458938	139647.300510	57.812711
2548.256861	139472.594916	57.817716
2547.436730	139329.065507	57.822721
2546.910709	139172.848440	57.827725
2546.127864	139009.126009	57.832730
2545.299951	138849.883824	57.837735
2544.891006	138699.596681	57.842740
2544.113194	138545.785950	57.847745
2543.584618	138369.067655	57.852749
2543.176555	138221.209432	57.857754
2542.142037	138062.868144	57.862759
2542.000535	137903.382498	57.867764
2540.846270	137737.566149	57.872769
2540.208273	137579.024859	57.877773
2539.837664	137418.853980	57.882778
2539.100205	137254.003358	57.887783
2538.676331	137088.214655	57.892788
2537.686039	136929.237231	57.897793
2537.207352	136760.803865	57.902797
2536.495734	136600.615267	57.907802
2535.684297	136450.924239	57.912807
2535.149369	136274.511713	57.917812
2534.271458	136131.095940	57.922817
2533.636325	135957.013333	57.927821
2533.014688	135796.268620	57.932826
2532.328084	135632.625937	57.937831
2531.429693	135461.471768	57.942836
2530.726706	135310.156050	57.947841
2530.630618	135148.201007	57.952845
2529.766790	134998.513053	57.957850
2528.871921	134829.559756	57.962855
2528.644536	134667.628211	57.967860
2527.654524	134500.851480	57.972865
2527.084545	134345.708758	57.977869
2526.160116	134178.415373	57.982874
2525.669388	134019.552545	57.987879
2525.183401	133864.767492	57.992884
2524.265838	133710.864661	57.997889
2524.015392	133531.349669	58.002893
2523.280695	133384.368047	58.007898
2522.455421	133221.383463	58.012903
2522.254219	133046.703425	58.017908
2521.462837	132884.922137	58.022913
2520.279726	132727.471879	58.027917
2520.287654	132560.560978	58.032922
2519.534462	132396.604306	58.037927
2518.937963	132226.666399	58.042932
2518.101528	132073.763024	58.047937
2517.363826	131888.860978	58.052941
2516.620354	131731.473587	58.057946
2516.000586	131565.544468	58.062951
2515.472263	131397.417110	58.067956
2514.443826	131244.002478	58.072961
2513.732920	131074.203949	58.077965
2513.078322	130909.160632	58.082970
2512.535294	130757.081600	58.087975
2511.720717	130579.262402	58.092980
2510.890321	130437.302933	58.097985
2510.471985	130269.558632	58.102989
2509.670035	130102.650918	58.107994
2509.151217	129955.195665	58.112999
2508.757141	129779.474104	58.118004
2507.847171	129628.653272	58.123009
2507.325392	129467.560136	58.128013
2506.720661	129302.696211	58.133018
2506.104072	129135.790309	58.138023
2505.620559	128978.021562	58.143028
2504.854342	128815.815181	58.148033
2504.223474	128641.167103	58.153037
2503.595311	128484.313138	58.158042
2502.661873	128317.830702	58.163047
2502.305462	128145.745846	58.168052
2501.285783	127981.742982	58.173057
2500.559858	127816.068905	58.178061
2500.050688	127647.808739	58.183066
2499.384232	127490.852198	58.188071
2498.582579	127334.248184	58.193076
2497.868825	127170.798571	58.198081
2497.523169	127001.830653	58.203085
2496.921714	126840.841680	58.208090
2495.915506	126687.143942	58.213095
2495.234194	126517.089251	58.218100
2495.024923	126355.990175	58.223105
2494.125707	126187.165840	58.228109
2493.264689	126024.889384	58.233114
2492.463619	125867.468235	58.238119
2492.285986	125694.087824	58.243124
2491.735180	125542.699126	58.248129
2490.953564	125365.200433	58.253133
2490.246054	125197.367798	58.258138
2489.346746	125033.744555	58.263143
2488.778028	124872.000127	58.268148
2487.872857	124715.402212	58.273153
2487.531283	124550.309329	58.278157
2486.949774	124384.823738	58.283162
2486.439394	124216.623100	58.288167
2485.699629	124043.304301	58.293172
2484.644743	123895.979375	58.298177
2484.244573	123724.640549	58.303181
2483.723292	123557.969570	58.308186
2482.937347	123398.998570	58.313191
2482.538802	123223.332628	58.318196
2481.345667	123062.917105	58.323201
2481.296965	122882.436205	58.328205
2480.198067	122728.699559	58.333210
2479.913744	122562.568644	58.338215
2479.053531	122380.480195	58.343220
2478.085711	122233.887126	58.348225
2477.633523	122059.494438	58.353229
2477.161557	121886.934465	58.358234
2476.122683	121728.597638	58.363239
2475.623909	121554.774348	58.368244
2474.887574	121396.378860	58.373249
2474.616673	121218.064951	58.378253
2473.898199	121062.004912	58.383258
2472.959464	120906.425109	58.388263
2472.845953	120718.490736	58.393268
2472.000167	120557.768730	58.398273
2471.187044	120385.082230	58.403277
2470.588857	120214.990999	58.408282
2469.782979	120059.477694	58.413287
2469.339308	119883.491972	58.418292
2468.558621	119715.458011	58.423297
2468.066630	119541.418456	58.428301
2467.329160	119366.688946	58.433306
2466.451265	119204.037847	58.438311
2465.916931	119023.520746	58.443316
2464.985257	118866.720469	58.448321
2464.559009	118693.126882	58.453325
2463.906672	118531.364700	58.458330
2463.369328	118366.055889	58.463335
2462.697959	118188.752958	58.468340
2461.800182	118018.145953	58.473345
2461.130925	117853.286639	58.478349
2460.747582	117683.482636	58.483354
2460.419593	117509.208579	58.488359
2459.992944	117331.879101	58.493364
2458.410250	117161.894162	58.498369
2457.935457	117005.007398	58.503373
2457.495007	116823.595817	58.508378
2456.566314	116651.758688	58.513383
2455.895210	116476.619319	58.518388
2455.183318	116310.773795	58.523393
2454.740539	116145.413516	58.528397
2454.204725	115984.734304	58.533402
2453.297331	115812.550357	58.538407
2452.987286	115636.134514	58.543412
2452.186188	115467.947474	58.548417
2451.506104	115288.952294	58.553421
2450.901232	115114.782912	58.558426
2450.249146	114949.641319	58.563431
2449.575214	114771.346997	58.568436
2448.706230	114589.156109	58.573441
2448.243971	114415.222819	58.578445
2447.596314	114248.396843	58.583450
2446.860523	114087.590015	58.588455
2446.372015	113905.305679	58.593460
2445.472689	113734.746692	58.598465
2444.773761	113561.865952	58.603469
2444.075846	113384.956139	58.608474
2443.464664	113211.035758	58.613479
2442.673454	113047.350350	58.618484
2442.220625	112882.298648	58.623489
2441.249953	112699.249102	58.628493
2440.941950	112534.805039	58.633498
2439.956378	112375.597338	58.638503
2439.816717	112189.874904	58.643508
2439.061765	112020.675548	58.648513
2438.253469	111856.048743	58.653517
2437.829393	111671.841252	58.658522
2437.079047	111500.683746	58.663527
2436.498257	111325.781732	58.668532
2435.814168	111164.884029	58.673537
2434.843835	110982.031142	58.678541
2434.297837	110811.937527	58.683546
2433.584926	110627.225171	58.688551
2433.221012	110458.152209	58.693556
2432.351162	110288.722755	58.698561
2431.509960	110110.900805	58.703565
2431.315005	109940.230869	58.708570
2430.456849	109770.606424	58.713575
2430.052462	109589.121002	58.718580
2429.028137	109415.648173	58.723585
2428.540175	109238.296902	58.728589
2427.829103	109055.233260	58.733594
2426.764346	108877.423999	58.738599
2426.366238	108697.073709	58.743604
2425.473413	108546.911974	58.748609
2424.927282	108373.345379	58.753613
2424.203141	108186.368938	58.758618
2423.512252	108029.642752	58.763623
2423.271413	107852.275105	58.768628
2422.137501	107690.564234	58.773633
2421.783837	107508.527928	58.778637
2421.225424	107338.600098	58.783642
2420.399013	107161.622230	58.788647
2419.954045	106978.563816	58.793652
2419.348986	106809.954174	58.798657
2418.305411	106647.049486	58.803661
2417.761241	106467.443271	58.808666
2416.783105	106296.028523	58.813671
2416.446409	106117.686370	58.818676
2415.308362	105953.595875	58.823681
2414.991891	105790.239125	58.828685
2414.618850	105610.104637	58.833690
2413.763134	105449.481410	58.838695
2413.292594	105270.843223	58.843700
2412.560424	105093.028225	58.848705
2411.491342	104914.493953	58.853709
2411.172952	104749.691767	58.858714
2410.378444	104576.985045	58.863719
2410.091587	104393.781790	58.868724
2409.094237	104239.083035	58.873729
2408.382676	104056.958454	58.878733
2407.995186	103878.133600	58.883738
2407.400423	103704.652967	58.888743
2406.841325	103533.382027	58.893748
2405.863118	103347.847686	58.898753
2405.121821	103175.815234	58.903757
2404.550890	103002.494591	58.908762
2403.635895	102848.071041	58.913767
2403.343965	102664.463323	58.918772
2402.415638	102499.633986	58.923777
2401.741568	102315.138026	58.928781
2401.492307	102141.252563	58.933786
2400.502433	101972.218160	58.938791
2399.882566	101799.345543	58.943796
2399.245101	101627.523681	58.948801
2398.436206	101444.254904	58.953805
2398.037278	101269.073880	58.958810
2397.006483	101095.852971	58.963815
2396.618085	100924.098305	58.968820
2395.707299	100762.145663	58.973825
2394.994564	100590.057953	58.978829
2394.534366	100417.753872	58.983834
2393.821290	100251.193664	58.988839
2393.314731	100070.412379	58.993844
2392.159388	99902.262916	58.998849
2391.408193	99735.997905	59.003853
2391.285026	99562.930001	59.008858
2390.477563	99402.575277	59.013863
2389.903056	99231.046644	59.018868
2389.257721	99066.241234	59.023873
2388.462375	98891.299653	59.028877
2388.091591	98707.279069	59.033882
2387.379235	98545.316885	59.038887
2386.947392	98365.095313	59.043892
2386.073635	98192.144065	59.048897
2385.283611	98024.793998	59.053901
2384.767173	97845.300303	59.058906
2384.092737	97684.023202	59.063911
2383.816044	97491.175148	59.068916
2382.719785	97325.496082	59.073921
2382.182163	97148.129585	59.078925
2381.893221	96964.477929	59.083930
2381.050173	96793.168739	59.088935
2380.189360	96619.421935	59.093940
2379.753775	96441.169570	59.098945
2379.251975	96258.908248	59.103949
2378.764787	96078.878463	59.108954
2377.618105	95897.832157	59.113959
2377.361481	95698.349815	59.118964
2376.465981	95532.220803	59.123969
2375.445791	95348.856765	59.128973
2375.044557	95171.693432	59.133978
2374.255282	95002.082564	59.138983
2373.815692	94824.940731	59.143988
2372.894327	94642.441942	59.148993
2372.553748	94466.479463	59.153997
2371.740989	94284.372232	59.159002
2370.463374	94125.645000	59.164007
2370.779636	93935.307959	59.169012
2369.889606	93751.600272	59.174017
2368.913859	93579.081044	59.179021
2368.632488	93394.645662	59.184026
2367.610496	93223.493551	59.189031
2367.237694	93037.661543	59.194036
2366.464617	92866.707336	59.199041
2365.768489	92678.500967	59.204045
2365.404426	92490.059656	59.209050
2364.289679	92313.311174	59.214055
2363.939764	92129.677114	59.219060
2363.666021	91959.322875	59.224065
2362.454162	91771.694248	59.229069
2362.083153	91586.298979	59.234074
2361.208495	91418.764372	59.239079
2360.423756	91243.684123	59.244084
2359.986545	91043.042057	59.249089
2359.173144	90862.053650	59.254093
2358.586452	90697.382840	59.259098
2357.703072	90506.251047	59.264103
2357.335476	90317.587959	59.269108
2356.910782	90157.346455	59.274113
2356.122106	89973.286429	59.279117
2355.588094	89783.170725	59.284122
2354.682893	89590.782365	59.289127
2354.162642	89422.927877	59.294132
2353.438588	89229.062110	59.299137
2352.642053	89023.841981	59.304141
2351.972831	88870.590997	59.309146
2351.178167	88685.040259	59.314151
2350.922174	88499.095042	59.319156
2350.238022	88314.138581	59.324161
2349.138922	88150.766510	59.329165
2348.390367	87964.092514	59.334170
2347.676995	87774.713879	59.339175
2347.306112	87603.584907	59.344180
2346.668447	87428.803663	59.349185
2345.678948	87248.076163	59.354189
2345.273059	87061.292260	59.359194
2344.247552	86887.673634	59.364199
2343.936348	86704.839912	59.369204
2343.385622	86530.153625	59.374209
2342.592983	86357.871642	59.379213
2341.878812	86169.762448	59.384218
2341.337270	85989.297826	59.389223
2340.648763	85815.406256	59.394228
2339.935877	85648.480172	59.399233
2339.415344	85456.809403	59.404237
2338.676575	85271.653292	59.409242
2337.783820	85114.959162	59.414247
2337.488755	84927.694584	59.419252
2336.616313	84741.486700	59.424257
2335.944865	84558.658777	59.429261
2335.511472	84372.390851	59.434266
2334.836048	84194.973527	59.439271
2334.455724	84013.245087	59.444276
2333.136111	83835.723764	59.449281
2332.746851	83641.937884	59.454285
2332.246673	83456.956295	59.459290
2330.996232	83301.447869	59.464295
2330.610465	83119.246287	59.469300
2330.305273	82930.498851	59.474305
2329.583843	82750.394585	59.479309
2329.093429	82565.007317	59.484314
2328.041026	82394.896671	59.489319
2327.509864	82199.441668	59.494324
2326.917495	82013.669819	59.499329
2325.964093	81841.595903	59.504333
2325.337607	81665.687904	59.509338
2324.639765	81481.743782	59.514343
2324.102903	81293.079538	59.519348
2323.632971	81114.793746	59.524353
2322.834988	80927.099521	59.529357
2322.502401	80741.183739	59.534362
2321.563385	80566.107770	59.539367
2321.102125	80378.447493	59.544372
2320.135101	80211.478154	59.549377
2319.180696	80031.022406	59.554381
2319.175378	79843.218626	59.559386
2318.396094	79658.467065	59.564391
2317.563077	79480.202214	59.569396
2317.362855	79292.966663	59.574401
2316.498662	79105.749389	59.579405
2316.015875	78921.394667	59.584410
2314.792882	78744.554137	59.589415
2314.228592	78574.422772	59.594420
2313.689468	78375.532498	59.599425
2312.894937	78194.585895	59.604429
2312.481442	78001.433073	59.609434
2311.633726	77829.274414	59.614439
2310.651418	77645.625028	59.619444
2310.243536	77450.227044	59.624449
2309.140722	77300.569845	59.629453
2308.958209	77101.521348	59.634458
2307.917461	76927.778794	59.639463
2307.466772	76759.792531	59.644468
2307.091542	76564.271138	59.649473
2306.010647	76398.934962	59.654477
2305.916592	76203.239392	59.659482
2304.718073	76043.804673	59.664487
2304.503280	75851.223642	59.669492
2303.940437	75677.739136	59.674497
2303.393735	75481.051552	59.679501
2302.542590	75313.571620	59.684506
2301.917958	75116.963300	59.689511
2301.330024	74917.829465	59.694516
2300.560244	74751.969571	59.699521
2299.783468	74567.371461	59.704525
2299.077754	74365.645169	59.709530
2298.312942	74199.149159	59.714535
2297.910722	73990.884636	59.719540
2297.139234	73830.145301	59.724545
2296.520693	73616.242495	59.729549
2295.832230	73453.345355	59.734554
2294.919867	73268.825050	59.739559
2294.376342	73108.606521	59.744564
2293.632518	72889.758281	59.749569
2292.686588	72742.390673	59.754573
2292.453835	72540.861169	59.759578
2291.599883	72360.907504	59.764583
2290.767955	72190.048803	59.769588
2290.327646	72016.443513	59.774593
2289.529446	71833.204369	59.779597
2289.207024	71665.164349	59.784602
2288.363695	71481.017090	59.789607
2287.680994	71285.120811	59.794612
2287.286182	71125.635826	59.799617
2286.694683	70922.044933	59.804621
2286.007469	70762.970314	59.809626
2284.928944	70568.759185	59.814631
2284.731599	70380.415094	59.819636
2283.695400	70197.007170	59.824641
2283.057557	70014.348548	59.829645
2282.786170	69844.555038	59.834650
2281.721522	69661.828036	59.839655
2281.426935	69477.251429	59.844660
2280.602978	69289.441550	59.849665
2279.748694	69121.995282	59.854669
2279.622538	68923.196684	59.859674
2279.083349	68734.681918	59.864679
2277.890663	68546.867981	59.869684
2277.043820	68365.682960	59.874689
2276.705443	68176.939057	59.879693
2276.108752	68003.159653	59.884698
2275.471575	67817.690370	59.889703
2274.476017	67635.262715	59.894708
2274.322591	67455.325200	59.899713
2273.573134	67277.694191	59.904718
2272.997358	67072.253546	59.909722
2271.958476	66887.461686	59.914727
2271.255122	66708.042648	59.919732
2270.565199	66523.886054	59.924737
2270.290298	66333.883408	59.929742
2269.397593	66163.603072	59.934746
2268.547602	65972.308298	59.939751
2268.096281	65769.350569	59.944756
2267.587413	65613.639734	59.949761
2266.659775	65418.920947	59.954766
2266.245448	65237.949917	59.959770
2265.577277	65053.968576	59.964775
2265.120874	64863.727434	59.969780
2264.464008	64675.736314	59.974785
2263.428538	64494.012784	59.979790
2262.872008	64301.320332	59.984794
2262.100075	64121.040301	59.989799
2261.495363	63935.824864	59.994804
2260.943151	63760.325830	59.999809
2260.460559	63562.984511	60.004814
2259.902306	63372.929501	60.009818
2258.849458	63198.876422	60.014823
2258.239464	63000.472056	60.019828
2257.257093	62822.020119	60.024833
2256.543858	62625.266485	60.029838
2256.430710	62446.778351	60.034842
2255.394063	62263.208476	60.039847
2254.906351	62075.539120	60.044852
2254.090530	61891.940989	60.049857
2253.381289	61714.760455	60.054862
2252.784123	61533.793486	60.059866
2252.038909	61337.482527	60.064871
2251.395654	61163.946691	60.069876
2250.520489	60990.417584	60.074881
2250.073079	60801.013447	60.079886
2249.692986	60620.707750	60.084890
2248.895360	60439.561514	60.089895
2248.026755	60244.889609	60.094900
2247.626811	60062.221498	60.099905
2247.010800	59884.271066	60.104910
2246.486873	59698.489259	60.109914
2245.389112	59517.165319	60.114919
2245.102670	59322.932947	60.119924
2244.184471	59141.042913	60.124929
2243.359184	58962.552049	60.129934
2242.770337	58777.182203	60.134938
2241.924832	58603.129289	60.139943
2241.307395	58414.909429	60.144948
2241.026834	58222.396783	60.149953
2240.155553	58051.223891	60.154958
2239.396625	57868.339870	60.159962
2238.897841	57690.705149	60.164967
2238.516151	57506.024102	60.169972
2237.656610	57320.838343	60.174977
2236.979100	57147.544702	60.179982
2236.694606	56946.658867	60.184986
2236.000312	56761.363890	60.189991
2235.032917	56579.870756	60.194996
2234.335100	56386.199627	60.200001
2233.650330	56196.481264	60.205006
2233.365095	56006.097019	60.210010
2232.472109	55834.207588	60.215015
2231.492159	55656.184593	60.220020
2231.169503	55462.602938	60.225025
2230.341726	55283.046730	60.230030
2230.131951	55090.042887	60.235034
2229.127123	54905.442485	60.240039
2228.277467	54716.626352	60.245044
2228.211878	54525.441017	60.250049
2227.241972	54348.482934	60.255054
2226.396265	54163.067361	60.260058
2225.885841	53971.967885	60.265063
2225.689419	53779.342853	60.270068
2224.780854	53595.588498	60.275073
2223.663118	53414.910064	60.280078
2223.588937	53214.914656	60.285082
2222.899052	53018.078918	60.290087
2221.806419	52839.952596	60.295092
2221.355765	52637.574195	60.300097
2220.547881	52454.198308	60.305102
2219.885594	52264.871685	60.310106
2219.004257	52084.861970	60.315111
2218.413805	51905.883678	60.320116
2218.137673	51711.144918	60.325121
2216.896496	51542.894978	60.330126
2216.796184	51345.072736	60.335130
2216.052261	51156.558529	60.340135
2215.200460	50958.049800	60.345140
2214.601620	50776.840899	60.350145
2213.930870	50594.781522	60.355150
2213.469587	50398.580393	60.360154
2212.868953	50223.850424	60.365159
2212.262689	50028.954493	60.370164
2211.413814	49844.776528	60.375169
2210.466260	49655.392968	60.380174
2210.054941	49464.622953	60.385178
2209.222356	49280.122386	60.390183
2208.205714	49089.382817	60.395188
2207.832844	48915.240096	60.400193
2207.404887	48734.100745	60.405198
2206.876326	48543.805248	60.410202
2205.997625	48354.348695	60.415207
2205.101797	48161.531066	60.420212
2204.750876	47978.482864	60.425217
2203.784456	47804.046628	60.430222
2203.255658	47614.140749	60.435226
2202.796118	47420.993102	60.440231
2202.269021	47237.252977	60.445236
2201.665140	47049.449627	60.450241
2200.691713	46866.957699	60.455246
2200.031084	46678.433460	60.460250
2198.883281	46499.398641	60.465255
2198.660813	46310.163575	60.470260
2197.920060	46119.538810	60.475265
2197.063760	45946.159944	60.480270
2196.851919	45760.171159	60.485274
2195.957810	45574.846086	60.490279
2195.051741	45389.562828	60.495284
2194.549545	45207.456202	60.500289
2193.918021	45019.185556	60.505294
2193.661781	44831.236936	60.510298
2193.021419	44647.633611	60.515303
2191.894095	44461.386390	60.520308
2191.862928	44268.037873	60.525313
2190.703838	44084.402595	60.530318
2190.556386	43886.965340	60.535322
2189.251650	43709.438796	60.540327
2188.392501	43519.272338	60.545332
2188.034571	43337.586152	60.550337
2187.277462	43156.262466	60.555342
2186.998537	42970.279302	60.560346
2186.165581	42800.963291	60.565351
2185.334403	42602.763653	60.570356
2185.068935	42409.498310	60.575361
2184.133019	42237.766002	60.580366
2183.447589	42043.942080	60.585370
2182.981242	41851.897534	60.590375
2182.491876	41661.050924	60.595380
2181.535783	41488.734794	60.600385
2180.786146	41303.024516	60.605390
2180.444692	41103.904330	60.610394
2179.555742	40921.575249	60.615399
2178.945788	40731.953343	60.620404
2178.227937	40544.266813	60.625409
2177.312680	40365.647339	60.630414
2177.192364	40177.666085	60.635418
2176.200912	39986.642671	60.640423
2175.239838	39812.601996	60.645428
2174.803986	39624.934571	60.650433
2173.813162	39437.981707	60.655438
2173.793697	39250.641241	60.660442
2172.875754	39080.517015	60.665447
2172.299264	38877.675482	60.670452
2171.897965	38696.306115	60.675457
2170.665599	38511.746107	60.680462
2170.167062	38321.790286	60.685466
2169.603777	38135.764004	60.690471
2168.766313	37943.545626	60.695476
2168.413381	37767.500899	60.700481
2167.229072	37593.761806	60.705486
2167.047229	37399.242080	60.710490
2166.215503	37223.933384	60.715495
2165.634856	37031.814246	60.720500
2165.077178	36846.063656	60.725505
2164.271008	36670.723463	60.730510
2163.627113	36475.913080	60.735514
2162.880964	36301.950242	60.740519
2162.335455	36110.258063	60.745524
2161.370223	35923.994339	60.750529
2161.049231	35746.372450	60.755534
2160.134346	35551.196942	60.760538
2159.367596	35380.422200	60.765543
2158.553213	35193.268644	60.770548
2158.156711	35006.591404	60.775553
2157.346666	34826.599226	60.780558
2156.845852	34652.671486	60.785562
2156.068190	34472.896084	60.790567
2155.402518	34292.452146	60.795572
2154.910903	34110.836765	60.800577
2153.969660	33940.087057	60.805582
2153.610795	33737.571664	60.810586
2152.762591	33581.775240	60.815591
2151.969039	33397.435739	60.820596
2151.819891	33202.079316	60.825601
2151.164516	33036.007587	60.830606
2150.441997	32843.214767	60.835610
2149.549987	32652.181456	60.840615
2148.893884	32472.891969	60.845620
2148.331328	32283.449347	60.850625
2147.582922	32104.341264	60.855630
2146.927595	31924.518757	60.860634
2146.237117	31757.428841	60.865639
2145.553011	31571.336762	60.870644
2144.633363	31382.956628	60.875649
2144.110090	31204.492577	60.880654
2143.521540	31026.415302	60.885658
2142.697629	30853.883867	60.890663
2142.026003	30678.225265	60.895668
2140.919729	30503.282163	60.900673
2140.363463	30329.317021	60.905678
2140.265586	30145.486518	60.910682
2139.597785	29969.669001	60.915687
2138.682811	29800.473187	60.920692
2138.379895	29615.540425	60.925697
2137.917863	29442.857420	60.930702
2137.087977	29256.998006	60.935706
2136.506886	29074.539108	60.940711
2135.627945	28896.305155	60.945716
2134.958760	28711.405996	60.950721
2134.213024	28534.632048	60.955726
2133.876534	28360.689346	60.960730
2133.064538	28179.571004	60.965735
2131.984565	27986.737169	60.970740
2131.458650	27814.247456	60.975745
2130.818366	27641.092105	60.980750
2130.436652	27468.974968	60.985754
2129.121849	27294.050452	60.990759
2128.760026	27124.850004	60.995764
2128.533875	26941.499395	61.000769
2127.351068	26767.376342	61.005774
2126.679711	26595.201516	61.010778
2126.080496	26417.226095	61.015783
2125.718659	26242.454004	61.020788
2124.747842	26073.253004	61.025793
2124.230184	25896.416405	61.030798
2123.417635	25700.037046	61.035802
2122.520998	25540.048297	61.040807
2122.020214	25366.963933	61.045812
2121.258094	25200.189674	61.050817
2120.674817	25028.038972	61.055822
2119.969377	24850.836171	61.060826
2119.474370	24678.371166	61.065831
2118.583794	24512.988323	61.070836
2118.192600	24332.866779	61.075841
2117.312297	24160.038103	61.080846
2117.026706	23995.727074	61.085850
2115.981694	23823.102706	61.090855
2115.008427	23649.017380	61.095860
2114.743512	23471.468585	61.100865
2114.187882	23314.215033	61.105870
2113.401346	23143.374052	61.110874
2112.654486	22977.261794	61.115879
2111.833989	22813.007570	61.120884
2110.987183	22641.871215	61.125889
2110.146620	22475.621937	61.130894
2109.684864	22308.955018	61.135898
2108.967138	22150.480056	61.140903
2108.385908	21988.423905	61.145908
2107.903249	21822.896130	61.150913
2106.994961	21661.426624	61.155918
2106.391034	21491.386958	61.160922
2105.731146	21343.804736	61.165927
2105.042656	21175.982424	61.170932
2104.450496	21004.337796	61.175937
2103.637743	20856.496993	61.180942
2103.143157	20686.008880	61.185946
2102.036169	20535.798630	61.190951
2101.447068	20370.766832	61.195956
2101.040821	20212.313231	61.200961
2100.110965	20060.544204	61.205966
2099.594924	19894.539851	61.210970
2098.807654	19752.397683	61.215975
2097.946161	19582.473593	61.220980
2097.468593	19428.007569	61.225985
2096.346298	19291.099346	61.230990
2096.025165	19134.613641	61.235994
2095.535059	18978.588539	61.240999
2094.620021	18839.966685	61.246004
2094.081985	18668.060346	61.251009
2092.837535	18528.046101	61.256014
2092.154176	18379.999321	61.261018
2091.589564	18234.666876	61.266023
2090.570620	18101.440841	61.271028
2089.826735	17956.611901	61.276033
2088.653360	17826.155112	61.281038
2088.032366	17700.208373	61.286042
2086.837883	17593.032037	61.291047
2085.588131	17471.136218	61.296052
2084.468946	17369.574975	61.301057
2083.219533	17278.988519	61.306062
2082.184997	17214.365982	61.311066
2080.826571	17137.532398	61.316071
2079.969267	17052.458916	61.321076
2079.448298	16988.178527	61.326081
2078.545176	16922.681092	61.331086
2078.115976	16857.101624	61.336090
2077.322313	16789.059505	61.341095
2076.741682	16717.969395	61.346100
2076.181770	16660.362515	61.351105
2075.187902	16595.906214	61.356110
2074.642696	16534.725345	61.361114
2074.274933	16484.521745	61.366119
2073.608958	16418.117598	61.371124
2073.015495	16338.449353	61.376129
2071.935431	16301.178729	61.381134
2071.624810	16229.845359	61.386138
2071.041361	16164.311069	61.391143
2070.058628	16119.189365	61.396148
2069.478587	16046.009405	61.401153
2068.838169	15990.776440	61.406158
2068.312685	15928.421944	61.411162
2068.036086	15878.468488	61.416167
2067.328268	15811.946712	61.421172
2066.749010	15737.600136	61.426177
2065.808015	15684.129715	61.431182
2065.393814	15615.211799	61.436186
2064.637678	15572.690465	61.441191
2063.815273	15512.179696	61.446196
2063.622871	15451.205431	61.451201
2062.896410	15390.533702	61.456206
2062.455055	15326.005988	61.461210
2061.678332	15262.981548	61.466215
2060.936479	15193.866234	61.471220
2060.441687	15140.521646	61.476225
2059.526332	15073.820828	61.481230
2059.244554	15013.050917	61.486234
2058.676305	14938.282334	61.491239
2057.974068	14883.325486	61.496244
2057.524254	14807.340178	61.501249
2056.418859	14744.457732	61.506254
2055.772858	14673.481353	61.511258
2054.854545	14623.777059	61.516263
2054.259616	14555.192093	61.521268
2053.969575	14493.250981	61.526273
2053.123467	14430.125058	61.531278
2052.403015	14381.626590	61.536282
2051.859785	14321.341098	61.541287
2051.171660	14267.490405	61.546292
2050.598465	14197.157557	61.551297
2049.978989	14132.147680	61.556302
2049.474181	14070.365183	61.561306
2048.678909	14017.495401	61.566311
2048.167698	13939.251738	61.571316
2047.693787	13863.069253	61.576321
2046.703812	13821.710548	61.581326
2046.412330	13737.681920	61.586330
2045.747926	13679.090870	61.591335
2045.009121	13611.731340	61.596340
2044.386194	13554.483955	61.601345
2043.470800	13484.278537	61.606350
2042.685442	13421.427693	61.611354
2041.965258	13363.265462	61.616359
2041.397962	13305.243237	61.621364
2041.007369	13238.689985	61.626369
2039.847006	13173.324749	61.631374
2039.609011	13120.433359	61.636378
2038.986457	13052.068748	61.641383
2038.273266	12997.050881	61.646388
2037.796406	12919.786225	61.651393
2036.710038	12870.076442	61.656398
2036.504372	12798.117768	61.661402
2035.782190	12744.904433	61.666407
2035.018760	12679.430977	61.671412
2034.414514	12617.005798	61.676417
2033.638449	12549.505270	61.681422
2033.221908	12489.283653	61.686426
2032.394977	12411.017547	61.691431
2031.602188	12367.628826	61.696436
2030.735401	12310.513722	61.701441
2030.204182	12244.634009	61.706446
2029.663383	12182.679732	61.711450
2029.294518	12118.150606	61.716455
2028.231977	12061.104991	61.721460
2028.035040	11994.011955	61.726465
2026.988157	11932.570458	61.731470
2026.457839	11874.071412	61.736474
2025.609074	11810.263461	61.741479
2024.933964	11749.990532	61.746484
2024.326055	11688.205362	61.751489
2023.551612	11630.800409	61.756494
2023.001380	11575.083820	61.761498
2022.221395	11506.775021	61.766503
2021.525188	11456.068768	61.771508
2021.138916	11391.786556	61.776513
2020.199234	11347.420779	61.781518
2019.659677	11288.010941	61.786522
2019.272161	11226.247122	61.791527
2018.168629	11171.005490	61.796532
2017.584347	11099.012185	61.801537
2016.861174	11044.971547	61.806542
2016.346411	10991.623944	61.811546
2015.706839	10929.908838	61.816551
2014.694563	10874.740602	61.821556
2014.815362	10813.409483	61.826561
2013.976718	10748.088479	61.831566
2013.217516	10690.734191	61.836570
2012.654101	10633.881442	61.841575
2011.873994	10568.345202	61.846580
2011.340304	10507.576440	61.851585
2010.630515	10452.620933	61.856590
2009.951578	10390.791983	61.861594
2009.339447	10333.022786	61.866599
2008.686979	10267.230105	61.871604
2008.070243	10216.446367	61.876609
2007.350682	10151.407293	61.881614
2006.827910	10086.584616	61.886618
2006.092594	10024.248933	61.891623
2005.311795	9961.068617	61.896628
2004.803547	9911.625358	61.901633
2004.006816	9849.548677	61.906638
2003.375467	9787.304381	61.911642
2002.705251	9723.534713	61.916647
2001.884964	9659.794657	61.921652
2001.537206	9585.839236	61.926657
2000.761186	9542.867431	61.931662
2000.045474	9480.780599	61.936666
1999.250646	9434.551301	61.941671
1998.571618	9386.034717	61.946676
1998.001389	9305.347109	61.951681
1997.305812	9252.015435	61.956686
1996.636875	9191.961817	61.961690
1996.070359	9143.032898	61.966695
1995.115312	9073.015803	61.971700
1994.765069	9012.821195	61.976705
1994.246113	8962.227360	61.981710
1993.560553	8902.470236	61.986714
1992.677234	8838.404041	61.991719
1992.345657	8779.835759	61.996724
1991.676116	8717.000015	62.001729
1990.847921	8653.516373	62.006734
1990.141064	8588.062352	62.011738
1989.705948	8526.312435	62.016743
1988.896627	8475.980916	62.021748
1988.373637	8412.851407	62.026753
1987.702896	8356.225686	62.031758
1986.796802	8300.571202	62.036762
1986.196467	8242.537590	62.041767
1985.456173	8181.074208	62.046772
1985.186072	8109.109256	62.051777
1984.343612	8056.715541	62.056782
1983.777242	7987.718670	62.061786
1983.310109	7932.787135	62.066791
1982.235441	7869.152279	62.071796
1981.963585	7803.595571	62.076801
1981.097426	7744.168363	62.081806
1980.423009	7671.995955	62.086810
1979.679547	7618.497849	62.091815
1978.786558	7563.623437	62.096820
1978.203666	7491.052412	62.101825
1977.372293	7449.953972	62.106830
1976.670689	7385.996908	62.111834
1976.230032	7326.487656	62.116839
1975.211961	7281.190287	62.121844
1975.040313	7222.009117	62.126849
1974.440606	7161.239559	62.131854
1973.651388	7103.636755	62.136858
1973.160431	7036.284936	62.141863
1972.154725	6985.366843	62.146868
1971.664724	6917.198180	62.151873
1970.932358	6867.514218	62.156878
1970.053909	6806.894479	62.161882
1969.725969	6742.286887	62.166887
1969.133789	6698.173976	62.171892
1968.390146	6636.954541	62.176897
1967.729228	6581.795287	62.181902
1967.201392	6526.142617	62.186906
1966.304351	6473.804164	62.191911
1965.594576	6416.092029	62.196916
1965.484652	6343.120230	62.201921
1964.673556	6293.841143	62.206926
1963.740291	6232.273278	62.211930
1963.429689	6157.613099	62.216935
1962.524531	6094.571831	62.221940
1961.871273	6037.816883	62.226945
1961.293351	5979.006465	62.231950
1960.621989	5910.461049	62.236954
1959.716948	5858.481780	62.241959
1958.859179	5802.760361	62.246964
1958.401314	5745.757816	62.251969
1957.708176	5700.890910	62.256974
1956.906509	5636.775065	62.261978
1956.410547	5588.939063	62.266983
1955.697976	5524.339462	62.271988
1955.293835	5455.072253	62.276993
1954.249570	5408.614270	62.281998
1953.803276	5340.333127	62.287002
1953.120935	5294.087015	62.292007
1952.599931	5236.270642	62.297012
1952.082658	5169.068723	62.302017
1951.316455	5117.275886	62.307022
1950.463831	5054.465760	62.312026
1949.935783	4989.281576	62.317031
1949.252782	4937.219039	62.322036
1948.767548	4878.153784	62.327041
1947.797598	4828.138168	62.332046
1947.115372	4763.710599	62.337050
1946.644122	4715.847475	62.342055
1945.474620	4663.742460	62.347060
1945.043439	4604.365280	62.352065
1944.506040	4540.932336	62.357070
1943.678316	4494.632154	62.362074
1943.005123	4434.607118	62.367079
1942.443053	4379.927807	62.372084
1941.658253	4319.663843	62.377089
1940.855615	4269.002871	62.382094
1940.631086	4215.937086	62.387098
1939.983298	4162.893728	62.392103
1939.024673	4103.288402	62.397108
1938.573079	4046.858486	62.402113
1938.049656	3989.685428	62.407118
1937.327231	3940.795257	62.412122
1936.665391	3883.542847	62.417127
1935.795224	3831.896439	62.422132
1935.382159	3781.854345	62.427137
1934.488467	3726.021092	62.432142
1933.903977	3666.769038	62.437146
1933.460345	3597.680867	62.442151
1932.521846	3553.724610	62.447156
1932.154142	3481.662760	62.452161
1931.641661	3424.761459	62.457166
1930.968830	3360.550693	62.462170
1929.992902	3317.303767	62.467175
1929.030399	3253.103969	62.472180
1928.282295	3196.505941	62.477185
1927.717652	3158.275345	62.482190
1927.041958	3095.320906	62.487194
1926.719561	3044.904953	62.492199
1925.895638	3001.733408	62.497204
1925.285622	2947.601731	62.502209
1924.584645	2896.826055	62.507214
1923.631670	2843.775196	62.512218
1923.085589	2785.544227	62.517223
1922.439345	2735.276175	62.522228
1921.744117	2683.284298	62.527233
1920.716147	2648.649705	62.532238
1920.430783	2590.081610	62.537242
1919.964972	2532.884586	62.542247
1919.089211	2493.618436	62.547252
1918.477836	2428.522724	62.552257
1917.901416	2389.526346	62.557262
1917.069289	2339.571480	62.562266
1916.728579	2277.725812	62.567271
1915.968289	2237.211835	62.572276
1915.404393	2181.123942	62.577281
1914.648096	2128.345698	62.582286
1914.107624	2090.308839	62.587290
1913.689626	2030.421895	62.592295
1912.803827	1980.907338	62.597300
1912.132873	1909.644988	62.602305
1911.486731	1868.020970	62.607310
1910.498395	1812.048406	62.612314
1909.660823	1749.252427	62.617319
1909.061981	1710.675416	62.622324
1908.611666	1654.961060	62.627329
1907.754618	1615.468786	62.632334
1907.235486	1555.101490	62.637338
1906.773237	1500.051209	62.642343
1906.079356	1449.881102	62.647348
1905.262745	1413.878541	62.652353
1904.348574	1352.664832	62.657358
1903.847171	1310.895631	62.662362
1903.296663	1268.214923	62.667367
1902.466352	1226.233238	62.672372
1901.989769	1173.009540	62.677377
1900.963014	1123.073194	62.682382
1900.246372	1080.673317	62.687386
1899.649268	1046.997638	62.692391
1898.634590	999.952073	62.697396
1898.055280	948.663169	62.702401
1897.322437	904.694091	62.707406
1897.022896	870.804417	62.712410
1896.615009	823.691474	62.717415
1895.860746	780.446865	62.722420
1895.162042	729.583769	62.727425
1894.366205	694.571629	62.732430
1893.325987	655.165461	62.737434
1892.920064	608.207451	62.742439
1892.043200	573.998537	62.747444
1891.339142	538.745119	62.752449
1890.859253	499.930090	62.757454
1890.038557	449.722077	62.762458
1889.398567	418.237191	62.767463
1888.521234	392.241602	62.772468
1887.915965	353.591952	62.777473
1887.499467	311.480991	62.782478
1886.383578	295.945520	62.787482
1886.112501	235.148517	62.792487
1885.261786	213.663811	62.797492
1884.815625	186.015315	62.802497
1883.620861	158.083608	62.807502
1883.127932	121.022064	62.812506
1882.417784	91.957001	62.817511
1881.466720	78.794105	62.822516
1880.476920	39.693847	62.827521
1879.363550	42.832163	62.832526
1878.370237	25.259070	62.837530
1878.050430	9.073983	62.842535
1876.363061	21.905284	62.847540
1875.371720	26.891295	62.852545
1874.303967	52.450913	62.857550
1873.819717	45.229894	62.862554
1873.870074	43.831143	62.867559
1873.242737	50.542867	62.872564
1873.077966	49.012695	62.877569
1872.109616	51.557145	62.882574
1870.794441	49.418011	62.887578
1871.026826	45.401054	62.892583
1870.405597	63.410459	62.897588
1869.891379	54.322387	62.902593
1869.217752	51.545239	62.907598
1868.150473	68.367089	62.912602
1867.503266	62.906552	62.917607
1866.617352	64.438148	62.922612
1865.613956	64.767858	62.927617
1865.539479	60.228772	62.932622
1864.766239	62.802171	62.937626
1864.749814	56.178638	62.942631
1864.008659	65.526134	62.947636
1863.324823	69.547146	62.952641
1862.640480	66.874199	62.957646
1861.675428	70.130901	62.962650
1861.067281	65.892587	62.967655
1860.348056	74.397683	62.972660
1859.587898	59.682773	62.977665
1858.829651	77.545221	62.982670
1858.027005	73.706788	62.987674
1858.690191	60.315997	62.992679
1857.129641	69.254291	62.997684
1856.143034	68.516916	63.002689
1856.185473	70.394690	63.007694
1855.599874	75.582801	63.012698
1854.769600	63.856254	63.017703
1853.639290	72.432930	63.022708
1853.285174	67.253859	63.027713
1852.955434	61.851727	63.032718
1852.189644	70.042524	63.037722
1851.048675	63.690583	63.042727
1850.472061	64.009304	63.047732
1850.410779	68.732547	63.052737
1849.897151	55.129655	63.057742
1848.275971	69.595231	63.062746
1847.918564	70.044723	63.067751
1847.555415	65.507319	63.072756
1846.912950	63.583074	63.077761
1845.783293	62.556186	63.082766
1845.315663	76.343453	63.087770
1845.555293	66.263643	63.092775
1843.792585	68.150505	63.097780
1842.919829	66.767442	63.102785
1842.658517	62.246985	63.107790
1842.255023	68.464295	63.112794
1841.801359	61.730420	63.117799
1840.902215	69.240662	63.122804
1840.122027	76.946482	63.127809
1839.145651	61.508988	63.132814
1839.024202	70.923667	63.137818
1838.718570	60.153018	63.142823
1837.185024	78.903384	63.147828
1836.270927	68.675614	63.152833
1836.564709	63.623901	63.157838
1835.836627	68.315830	63.162842
1834.931967	65.578528	63.167847
1833.981358	62.167293	63.172852
1833.399891	58.746329	63.177857
1832.942488	58.965701	63.182862
1832.402701	74.517961	63.187866
1831.880495	59.080895	63.192871
1830.957695	68.935049	63.197876
1830.557501	64.603800	63.202881
1829.932155	59.254919	63.207886
1828.815012	75.554858	63.212890
1828.681265	50.116772	63.217895
1828.017934	73.095448	63.222900
1827.370971	62.569807	63.227905
1826.770225	56.672985	63.232910
1825.414970	67.377962	63.237914
1824.765852	50.805175	63.242919
1824.574014	73.576522	63.247924
1823.855692	64.196020	63.252929
1823.150040	62.997738	63.257934
1822.267763	64.415232	63.262938
1821.643602	62.303587	63.267943
1820.958902	71.676822	63.272948
1820.634978	57.578622	63.277953
1819.923381	56.080093	63.282958
1819.422289	80.882748	63.287962
1819.059568	55.280746	63.292967
1818.433648	58.344839	63.297972
1817.051942	57.618181	63.302977
1816.108852	54.817607	63.307982
1815.376238	66.535445	63.312986
1815.709654	66.059974	63.317991
1814.549667	69.689838	63.322996
1813.610689	68.769878	63.328001
1813.193123	62.221084	63.333006
1812.542128	61.641741	63.338010
1812.316454	53.594366	63.343015
1811.523448	68.518216	63.348020
1810.940354	72.058051	63.353025
1810.463889	65.813494	63.358030
1808.932938	68.030999	63.363034
1808.389787	72.023377	63.368039
1807.575410	62.136174	63.373044
1807.868614	58.492745	63.378049
1807.311884	61.295123	63.383054
1806.039857	72.444202	63.388058
1805.831060	69.320448	63.393063
1804.722217	69.599119	63.398068
1804.019447	64.800270	63.403073
1803.009352	66.003106	63.408078
1802.058334	75.978445	63.413082
1802.617817	61.336270	63.418087
1801.430435	72.427755	63.423092
1800.608149	59.657622	63.428097
1800.049965	61.596079	63.433102
1799.183518	65.370142	63.438106
1798.990354	58.478219	63.443111
1798.201332	68.101406	63.448116
1797.520445	67.512620	63.453121
1796.857254	58.777800	63.458126
1796.465947	67.249753	63.463130
1795.685482	57.087521	63.468135
1794.792206	69.832223	63.473140
1794.173960	63.297956	63.478145
1793.762059	61.315034	63.483150
1793.208400	64.523774	63.488154
1792.428049	62.922632	63.493159
1791.077481	63.913041	63.498164
1790.270269	58.249285	63.503169
1790.164505	57.643286	63.508174
1789.714983	64.790407	63.513178
1789.133348	71.229974	63.518183
1788.366162	72.726972	63.523188
1787.641132	59.488823	63.528193
1787.354261	64.000310	63.533198
1786.356258	66.341347	63.538202
1785.391058	54.440728	63.543207
1784.435564	74.487000	63.548212
1784.279184	64.132620	63.553217
1783.965860	63.956967	63.558222
1782.982874	74.676963	63.563226
1782.402638	62.246858	63.568231
1781.762092	54.757372	63.573236
1781.268620	63.858970	63.578241
1780.742900	54.660789	63.583246
1779.290726	53.678843	63.588250
1778.641524	56.838102	63.593255
1777.999272	68.126867	63.598260
1777.340670	66.881702	63.603265
1776.954719	49.286299	63.608270
1776.781829	69.558358	63.613274
1776.238740	58.718204	63.618279
1775.755473	60.471307	63.623284
1774.543212	67.312216	63.628289
1773.975036	58.428277	63.633294
1773.206934	70.145453	63.638298
1772.891558	54.459528	63.643303
1772.012776	62.250397	63.648308
1770.792828	65.241686	63.653313
1770.134231	62.173601	63.658318
1769.195161	69.303857	63.663322
1769.058671	56.823790	63.668327
1768.495301	57.481040	63.673332
1768.217161	69.964057	63.678337
1767.768276	62.571864	63.683342
1766.695573	58.292240	63.688346
1765.994655	55.951532	63.693351
1764.868580	69.755057	63.698356
1764.466517	61.702583	63.703361
1763.737990	67.009597	63.708366
1763.397131	68.826818	63.713370
1763.044799	62.534176	63.718375
1762.170986	57.915468	63.723380
1760.984870	71.954031	63.728385
1760.711812	54.373813	63.733390
1759.540207	68.206646	63.738394
1759.144227	54.690755	63.743399
1758.540601	64.172542	63.748404
1758.338586	63.316907	63.753409
1757.477079	53.774678	63.758414
1756.110562	67.002966	63.763418
1756.018116	43.769201	63.768423
1755.309507	66.841789	63.773428
1755.020727	58.176828	63.778433
1754.783831	50.489209	63.783438
1753.321916	59.695728	63.788442
1752.899909	53.310081	63.793447
1752.022009	68.036114	63.798452
1751.699240	67.980234	63.803457
1751.333425	51.073908	63.808462
1749.603505	72.834289	63.813466
1748.692077	52.589542	63.818471
1748.400855	63.190211	63.823476
1747.771457	68.889908	63.828481
1747.612892	59.423692	63.833486
1746.825680	64.249607	63.838490
1746.613784	58.494473	63.843495
1745.896414	42.684761	63.848500
1744.863057	60.489969	63.853505
1743.935394	59.295431	63.858510
1743.409736	68.247610	63.863514
1743.089711	63.441608	63.868519
1742.302591	59.461984	63.873524
1741.166974	63.140044	63.878529
1740.691524	52.610856	63.883534
1740.050774	60.018582	63.888538
1739.650824	53.224166	63.893543
1738.967526	61.070726	63.898548
1738.334254	72.082111	63.903553
1737.547282	60.457550	63.908558
1736.437998	70.300346	63.913562
1736.006921	60.328644	63.918567
1735.326399	70.212150	63.923572
1734.774403	59.436501	63.928577
1734.928739	55.220623	63.933582
1733.706505	67.134507	63.938586
1732.754633	60.457711	63.943591
1731.947610	53.773681	63.948596
1731.579283	56.916725	63.953601
1731.021841	60.632267	63.958606
1730.398949	57.832908	63.963610
1729.926354	61.683204	63.968615
1728.780583	67.843380	63.973620
1727.737718	58.591734	63.978625
1727.718728	62.723216	63.983630
1727.019216	58.546761	63.988634
1726.568602	51.489165	63.993639
1726.356154	54.077606	63.998644
1725.140367	67.524813	64.003649
1724.373713	61.905099	64.008654
1723.556318	63.548858	64.013658
1723.489466	66.224561	64.018663
1722.398799	63.568884	64.023668
1721.211371	69.530680	64.028673
1720.899788	56.985393	64.033678
1720.157661	68.941296	64.038682
1719.769210	60.352096	64.043687
1719.575696	67.214141	64.048692
1718.519267	63.078607	64.053697
1717.817117	65.454677	64.058702
1716.896734	61.581381	64.063706
1716.512389	60.459826	64.068711
1716.065008	60.986703	64.073716
1715.025977	57.259985	64.078721
1714.091441	55.588743	64.083726
1713.534182	65.347017	64.088730
1713.141613	57.431820	64.093735
1712.318895	56.051895	64.098740
1711.749799	59.513830	64.103745
1711.417349	63.698254	64.108750
1710.296493	59.684919	64.113754
1710.091356	60.556512	64.118759
1709.268026	60.130721	64.123764
1708.589348	56.848230	64.128769
1708.293271	47.578908	64.133774
1706.876547	61.767644	64.138778
1706.061759	62.102150	64.143783
1705.414146	59.013417	64.148788
1704.870906	51.934270	64.153793
1704.830192	44.232847	64.158798
1704.215445	67.806181	64.163802
1703.856300	63.984090	64.168807
1702.310853	58.842895	64.173812
1701.677945	47.173389	64.178817
1701.260436	48.506059	64.183822
1700.898442	52.119598	64.188826
1700.217658	61.413378	64.193831
1699.142282	58.859360	64.198836
1698.578315	59.601873	64.203841
1698.200568	46.073652	64.208846
1697.538500	56.862528	64.213850
1696.621345	60.110098	64.218855
1695.666362	47.963484	64.223860
1695.296341	60.653469	64.228865
1694.875125	52.093138	64.233870
1694.340596	55.494393	64.238874
1693.333214	70.559543	64.243879
1692.220389	62.053870	64.248884
1691.270039	62.200184	64.253889
1691.207421	59.105264	64.258894
1690.393051	65.159196	64.263898
1689.972680	59.692646	64.268903
1689.603605	60.405781	64.273908
1689.145521	54.905800	64.278913
1688.202620	51.255287	64.283918
1687.356694	59.159226	64.288922
1686.406066	56.668975	64.293927
1686.389741	44.963037	64.298932
1685.557045	67.639031	64.303937
1684.580046	53.542110	64.308942
1683.644565	60.446317	64.313946
1682.939514	67.482655	64.318951
1682.625653	55.412394	64.323956
1682.236723	53.301268	64.328961
1682.100617	54.046782	64.333966
1681.224395	53.842287	64.338970
1680.343234	54.294574	64.343975
1679.587839	54.361039	64.348980
1678.567260	46.078845	64.353985
1677.860289	52.954636	64.358990
1677.181702	57.843735	64.363994
1676.744562	58.580299	64.368999
1676.113980	56.614790	64.374004
1675.725395	65.193547	64.379009
1675.574366	56.244954	64.384014
1674.431980	66.644947	64.389018
1673.630089	55.803363	64.394023
1672.710639	56.548734	64.399028
1672.378740	63.145760	64.404033
1671.538306	51.064536	64.409038
1670.239168	49.214691	64.414042
1669.923435	59.909135	64.419047
1669.448353	57.270813	64.424052
1668.925843	57.521056	64.429057
1668.688313	49.153900	64.434062
1667.769447	72.056474	64.439066
1666.931397	66.347198	64.444071
1666.151945	58.233277	64.449076
1665.834104	52.252141	64.454081
1665.262156	49.756939	64.459086
1664.162145	53.866177	64.464090
1663.535790	62.358127	64.469095
1663.394513	52.945952	64.474100
1662.586920	60.782308	64.479105
1661.559583	56.093412	64.484110
1660.354180	60.243050	64.489114
1659.933803	54.300279	64.494119
1659.725148	59.993075	64.499124
1658.899448	62.984861	64.504129
1658.875858	63.535889	64.509134
1657.893755	68.640363	64.514138
1656.994049	53.298028	64.519143
1656.458615	61.393920	64.524148
1655.721528	60.013026	64.529153
1655.346043	60.634146	64.534158
1653.888419	61.173285	64.539162
1653.538184	53.989377	64.544167
1653.004256	48.018919	64.549172
1652.490387	63.849324	64.554177
1652.069105	55.587050	64.559182
1651.082676	51.164470	64.564186
1650.382200	60.213808	64.569191
1649.702475	60.192569	64.574196
1649.147168	61.163947	64.579201
1649.063235	43.175273	64.584206
1647.866297	52.057474	64.589210
1646.805977	52.774771	64.594215
1646.372447	54.396995	64.599220
1645.866209	57.459456	64.604225
1645.752189	57.723658	64.609230
1644.222723	57.919409	64.614234
1643.706084	53.765968	64.619239
1643.280319	48.609365	64.624244
1642.368367	57.555106	64.629249
1642.346512	47.404892	64.634254
1641.187506	53.573504	64.639258
1640.745284	49.133860	64.644263
1639.746951	51.065000	64.649268
1639.355467	49.898862	64.654273
1638.826070	61.374709	64.659278
1637.896726	57.578562	64.664282
1637.314014	61.624557	64.669287
1637.047925	56.852584	64.674292
1635.973249	58.321203	64.679297
1635.008947	50.364394	64.684302
1634.231300	57.182039	64.689306
1634.073348	56.929683	64.694311
1633.373034	60.268979	64.699316
1632.193139	55.336256	64.704321
1631.456637	52.640128	64.709326
1631.219133	53.650906	64.714330
1630.662993	52.266504	64.719335
1630.304017	54.067693	64.724340
1629.700302	60.165442	64.729345
1628.748519	53.185912	64.734350
1627.939846	60.473680	64.739354
1627.526963	53.886343	64.744359
1627.141523	55.418930	64.749364
1626.042500	59.725143	64.754369
1625.381698	47.364676	64.759374
1624.652417	59.872043	64.764378
1624.616271	58.335648	64.769383
1623.111453	60.670528	64.774388
1622.391249	60.685689	64.779393
1622.011957	52.301638	64.784398
1621.394044	59.467641	64.789402
1620.667913	51.704807	64.794407
1620.033301	53.120865	64.799412
1619.054946	62.277433	64.804417
1618.381485	56.102071	64.809422
1618.012016	51.486874	64.814426
1617.919906	51.509480	64.819431
1617.273407	54.185808	64.824436
1615.922810	61.496598	64.829441
1615.604291	50.505711	64.834446
1615.122531	59.509269	64.839450
1613.868551	53.388292	64.844455
1613.097939	51.586970	64.849460
1612.170342	49.750665	64.854465
1612.335276	58.470136	64.859470
1611.438836	55.398885	64.864474
1611.243627	45.173718	64.869479
1610.489041	52.031856	64.874484
1609.311820	52.657356	64.879489
1608.941092	51.849039	64.884494
1608.527361	59.055142	64.889498
1607.535879	57.164335	64.894503
1606.678769	51.070195	64.899508
1605.770108	53.526407	64.904513
1605.478859	59.016288	64.909518
1605.263743	59.091553	64.914522
1604.423004	46.846413	64.919527
1603.194322	47.882205	64.924532
1602.184819	46.025803	64.929537
1602.129109	48.054773	64.934542
1601.441575	50.283471	64.939546
1601.201510	65.188882	64.944551
1600.891360	51.508022	64.949556
1599.765491	52.705673	64.954561
1599.663555	53.349570	64.959566
1598.401695	53.168526	64.964570
1597.377372	53.323472	64.969575
1596.513617	57.392047	64.974580
1595.906358	64.732978	64.979585
1595.992665	60.267714	64.984590
1595.627170	52.204747	64.989594
1594.663658	55.276791	64.994599
1593.842662	55.446741	64.999604
1592.945147	58.531955	65.004609
1592.386010	43.909821	65.009614
1591.183892	58.887652	65.014618
1590.668514	52.501109	65.019623
1590.438137	40.955349	65.024628
1589.760924	55.580128	65.029633
1589.407421	48.625408	65.034638
1588.348394	59.232948	65.039642
1587.894838	54.210078	65.044647
1587.427864	44.058056	65.049652
1586.254458	59.690479	65.054657
1585.530432	54.604929	65.059662
1584.594879	54.542353	65.064666
1584.226891	57.135015	65.069671
1584.214153	44.988561	65.074676
1583.262071	70.605560	65.079681
1582.842236	56.745013	65.084686
1581.813036	59.493192	65.089690
1581.184662	58.557084	65.094695
1580.772351	49.452910	65.099700
1579.348057	45.380623	65.104705
1579.004629	60.460142	65.109710
1578.191807	52.111868	65.114714
1578.044419	44.645022	65.119719
1577.611733	57.110000	65.124724
1576.296926	61.072056	65.129729
1575.914525	53.245163	65.134734
1575.109627	60.240613	65.139738
1574.646796	66.232413	65.144743
1573.997798	51.883170	65.149748
1572.966478	61.048165	65.154753
1572.333860	61.013154	65.159758
1571.933673	60.280484	65.164762
1571.297194	64.861725	65.169767
1570.769528	44.294349	65.174772
1569.722466	56.234062	65.179777
1569.544275	51.362982	65.184782
1568.889423	59.581935	65.189786
1567.583312	61.669236	65.194791
1567.099027	57.980593	65.199796
1566.354795	53.857026	65.204801
1566.127202	53.057511	65.209806
1565.578791	52.154433	65.214810
1564.691174	51.693173	65.219815
1563.946765	55.928871	65.224820
1563.154428	60.761953	65.229825
1562.909523	57.639235	65.234830
1561.761979	44.950867	65.239834
1561.129529	53.432756	65.244839
1560.631857	43.361312	65.249844
1559.710207	51.669960	65.254849
1559.748092	47.270741	65.259854
1559.025926	55.099851	65.264858
1557.861357	51.492497	65.269863
1557.484620	55.029548	65.274868
1556.645572	58.668442	65.279873
1556.235352	49.611249	65.284878
1554.915507	55.922143	65.289882
1554.286372	45.147783	65.294887
1554.102093	46.427647	65.299892
1553.612287	53.037150	65.304897
1553.225498	51.953856	65.309902
1552.129170	50.573307	65.314906
1551.643350	49.912593	65.319911
1551.285971	56.428517	65.324916
1549.559851	58.757602	65.329921
1548.836048	56.728093	65.334926
1548.137661	47.238887	65.339930
1547.721397	41.169341	65.344935
1547.440806	49.317784	65.349940
1546.848101	57.279287	65.354945
1547.053871	49.328983	65.359950
1545.850484	56.882909	65.364954
1544.867888	57.725089	65.369959
1544.551475	46.278159	65.374964
1543.061342	63.055304	65.379969
1542.660625	50.215157	65.384974
1542.205806	52.299661	65.389978
1541.634848	45.347968	65.394983
1541.296491	46.053088	65.399988
1540.055949	49.757359	65.404993
1539.824467	47.466702	65.409998
1539.389897	43.718132	65.415002
1538.242512	56.537944	65.420007
1537.468252	45.376653	65.425012
1536.518098	51.163619	65.430017
1536.426429	46.876448	65.435022
1535.485566	53.496126	65.440026
1534.421152	51.151748	65.445031
1534.065165	49.418605	65.450036
1533.455249	59.951642	65.455041
1533.161444	52.159566	65.460046
1532.919393	53.483304	65.465050
1531.667383	52.327769	65.470055
1531.561787	54.869281	65.475060
1529.852103	48.183691	65.480065
1529.071720	45.128724	65.485070
1528.530309	48.739251	65.490074
1528.379854	41.656091	65.495079
1527.966063	49.931354	65.500084
1527.131515	61.298008	65.505089
1526.901920	49.351594	65.510094
1525.714747	53.708119	65.515098
1524.945215	59.698196	65.520103
1524.656951	51.607204	65.525108
1523.360016	59.661695	65.530113
1523.032340	48.596596	65.535118
1522.280119	52.589122	65.540122
1521.370701	60.127884	65.545127
1521.616921	51.045232	65.550132
1520.073968	57.595018	65.555137
1519.761350	53.521148	65.560142
1518.980402	52.650302	65.565146
1518.895826	58.738111	65.570151
1518.084308	48.948355	65.575156
1516.955120	58.669800	65.580161
1516.258431	49.954600	65.585166
1515.586210	55.071372	65.590170
1514.675378	56.127658	65.595175
1513.983428	52.044685	65.600180
1513.308111	53.799965	65.605185
1512.901046	56.296345	65.610190
1512.639994	56.047765	65.615194
1512.294752	50.533050	65.620199
1511.869469	52.705903	65.625204
1510.505982	58.121757	65.630209
1510.143776	44.179548	65.635214
1508.791631	51.055398	65.640218
1507.825965	48.987069	65.645223
1507.447502	59.688328	65.650228
1507.045347	54.149541	65.655233
1506.979677	48.361748	65.660238
1506.556404	49.996554	65.665242
1505.044421	47.734352	65.670247
1504.628359	48.382440	65.675252
1503.771627	58.814358	65.680257
1503.407157	50.812749	65.685262
1502.188579	60.849596	65.690266
1501.418349	51.956857	65.695271
1501.367563	54.032353	65.700276
1501.118619	50.367828	65.705281
1500.375612	59.200028	65.710286
1499.307423	46.846005	65.715290
1498.612680	53.937503	65.720295
1498.101483	42.978847	65.725300
1496.803747	51.380394	65.730305
1496.494557	48.398787	65.735310
1495.931535	45.843863	65.740314
1494.977489	51.749729	65.745319
1495.144006	53.511577	65.750324
1493.906010	50.876265	65.755329
1493.325467	48.199550	65.760334
1492.791507	50.660905	65.765338
1492.260552	45.467438	65.770343
1491.146389	48.874109	65.775348
1490.476007	52.629716	65.780353
1490.102145	47.740859	65.785358
1489.815308	51.252591	65.790362
1488.631219	51.412470	65.795367
1488.218421	43.465857	65.800372
1486.927670	51.352223	65.805377
1486.749665	47.603889	65.810382
1486.204587	58.881970	65.815386
1485.389079	42.395706	65.820391
1484.854805	41.654399	65.825396
1484.232012	54.646318	65.830401
1483.329437	47.225384	65.835406
1482.394434	53.574495	65.840410
1481.641587	61.331230	65.845415
1481.398145	55.589034	65.850420
1480.901561	56.098539	65.855425
1480.451930	52.487987	65.860430
1479.505771	52.189021	65.865434
1478.420954	62.171505	65.870439
1477.896959	46.517254	65.875444
1477.452521	58.014301	65.880449
1477.223451	47.884423	65.885454
1476.064510	54.161895	65.890458
1475.515721	54.990350	65.895463
1475.310136	48.996142	65.900468
1473.986907	51.043631	65.905473
1473.424664	48.069129	65.910478
1472.618792	48.746058	65.915482
1472.409626	52.526138	65.920487
1471.765523	47.006890	65.925492
1470.736648	46.159692	65.930497
1470.204901	52.223950	65.935502
1469.604874	50.054950	65.940506
1468.838464	42.475192	65.945511
1468.049866	40.597930	65.950516
1467.341078	46.247210	65.955521
1466.684631	47.054930	65.960526
1466.189886	42.995826	65.965530
1465.564495	56.945348	65.970535
1465.296753	41.529495	65.975540
1464.102183	45.477222	65.980545
1463.782843	49.918192	65.985550
1463.195986	49.554245	65.990554
1462.122593	58.550920	65.995559
1461.507411	51.475393	66.000564
1460.690074	57.838927	66.005569
1460.715707	42.184065	66.010574
1459.922092	63.489826	66.015578
1458.880410	51.158417	66.020583
1458.441197	38.696575	66.025588
1457.524047	64.782674	66.030593
1457.287570	47.933162	66.035598
1456.354765	61.144667	66.040602
1455.762939	65.873372	66.045607
1455.277454	44.121386	66.050612
1453.797829	65.026836	66.055617
1453.518391	45.031902	66.060622
1452.923580	40.033095	66.065626
1452.037839	51.466238	66.070631
1452.172637	44.129598	66.075636
1451.073724	60.280063	66.080641
1450.427842	43.336359	66.085646
1450.253810	52.874476	66.090650
1449.244536	56.073689	66.095655
1448.662535	47.822823	66.100660
1447.590337	54.559593	66.105665
1447.311987	42.240915	66.110670
1446.179083	51.633394	66.115674
1445.225374	54.442163	66.120679
1445.218285	46.796921	66.125684
1444.346351	55.375237	66.130689
1444.203529	56.722634	66.135694
1443.466124	49.456810	66.140698
1442.242103	56.124675	66.145703
1442.225447	43.124178	66.150708
1441.353901	44.319320	66.155713
1440.563978	53.371868	66.160718
1439.339508	53.933993	66.165722
1438.685259	55.335868	66.170727
1438.718448	45.599544	66.175732
1438.112877	53.897412	66.180737
1437.137901	51.169863	66.185742
1436.272525	45.547028	66.190746
1435.635810	58.244708	66.195751
1435.590297	41.820586	66.200756
1434.654901	48.630229	66.205761
1433.759943	47.528378	66.210766
1433.398414	50.241452	66.215770
1432.695256	37.080422	66.220775
1431.550683	48.203054	66.225780
1430.994714	54.594436	66.230785
1430.659123	50.275081	66.235790
1430.322550	40.621186	66.240794
1428.857228	53.283410	66.245799
1428.632491	44.777076	66.250804
1427.927366	44.558088	66.255809
1427.561790	44.740859	66.260814
1426.916230	51.050287	66.265818
1425.545489	55.068610	66.270823
1425.393709	45.823723	66.275828
1424.807336	53.656506	66.280833
1424.247944	46.043859	66.285838
1423.142047	32.789159	66.290842
1422.154365	46.370493	66.295847
1421.988320	50.063298	66.300852
1421.443971	58.753553	66.305857
1420.616736	52.556970	66.310862
1419.978753	48.673602	66.315866
1419.040225	44.880583	66.320871
1419.075956	44.313611	66.325876
1418.480395	51.840356	66.330881
1417.426429	40.606886	66.335886
1416.743771	43.650116	66.340890
1416.045541	47.962084	66.345895
1415.526846	43.249225	66.350900
1414.642057	48.016612	66.355905
1413.973868	48.386253	66.360910
1413.810949	41.153707	66.365914
1412.405903	47.104474	66.370919
1412.165722	39.710749	66.375924
1411.329504	57.752760	66.380929
1410.959851	53.014632	66.385934
1410.703922	44.055956	66.390938
1409.258464	62.906001	66.395943
1408.878141	47.052324	66.400948
1408.168973	43.809465	66.405953
1407.479701	51.980295	66.410958
1406.508120	50.638326	66.415962
1405.999887	43.772897	66.420967
1405.438495	51.712094	66.425972
1405.091021	58.048263	66.430977
1404.073586	52.402301	66.435982
1403.648395	45.632478	66.440986
1402.849531	57.392441	66.445991
1402.912771	46.148544	66.450996
1401.463109	50.403344	66.456001
1400.737121	43.552029	66.461006
1400.218318	50.254464	66.466010
1399.636434	42.142367	66.471015
1398.463545	54.406470	66.476020
1397.697521	53.662596	66.481025
1397.248409	50.297979	66.486030
1397.224273	46.160930	66.491034
1396.733499	55.687896	66.496039
1395.794640	42.092845	66.501044
1394.699052	50.774529	66.506049
1394.514536	45.291060	66.511054
1393.860727	44.485197	66.516058
1392.796395	49.863012	66.521063
1392.247693	47.957102	66.526068
1391.622706	48.769302	66.531073
1390.953694	41.251362	66.536078
1390.016343	37.833474	66.541082
1389.357447	46.007360	66.546087
1389.058977	46.993156	66.551092
1388.574030	53.934635	66.556097
1387.841650	43.228787	66.561102
1386.985180	35.122500	66.566106
1385.960913	52.432753	66.571111
1386.152447	33.454215	66.576116
1385.023325	51.511244	66.581121
1384.023217	45.260159	66.586126
1383.723504	43.806669	66.591130
1383.251367	51.832604	66.596135
1382.833776	36.126795	66.601140
1381.912700	44.099513	66.606145
1381.016465	38.628261	66.611150
1380.466599	35.456280	66.616154
1379.288172	44.573747	66.621159
1378.691398	34.352542	66.626164
1377.967503	48.696181	66.631169
1377.589400	45.115282	66.636174
1377.192597	45.066487	66.641178
1376.996538	39.125976	66.646183
1375.848959	41.853623	66.651188
1375.071303	42.182329	66.656193
1374.423961	39.158305	66.661198
1373.968848	30.737496	66.666202
1372.908749	41.715831	66.671207
1372.584630	33.871846	66.676212
1372.035639	43.067447	66.681217
1370.994031	52.092211	66.686222
1370.423807	42.623701	66.691226
1369.664013	39.496132	66.696231
1369.391392	47.266428	66.701236
1368.786654	44.836436	66.706241
1367.678981	44.247805	66.711246
1366.961991	41.395699	66.716250
1366.376344	42.297842	66.721255
1366.304174	39.024696	66.726260
1365.263867	41.804679	66.731265
1364.552070	52.183621	66.736270
1363.955360	32.661782	66.741274
1362.937127	39.224421	66.746279
1362.482713	42.824298	66.751284
1361.436143	52.035929	66.756289
1361.071123	38.002757	66.761294
1360.811849	34.874471	66.766298
1360.158459	41.735494	66.771303
1359.537380	49.865530	66.776308
1358.824304	46.725805	66.781313
1358.452568	44.738157	66.786318
1357.441268	40.237661	66.791322
1356.351119	49.196028	66.796327
1356.107269	43.792958	66.801332
1355.067857	44.712047	66.806337
1353.907406	47.998401	66.811342
1353.838200	47.684648	66.816346
1353.103103	54.394668	66.821351
1353.011162	43.889790	66.826356
1352.202617	40.995475	66.831361
1351.615232	34.087456	66.836366
1350.685691	44.658701	66.841370
1350.139530	45.977183	66.846375
1349.431364	37.951410	66.851380
1348.526871	58.951532	66.856385
1348.048768	58.218671	66.861390
1347.772916	39.948352	66.866394
1346.640156	58.406512	66.871399
1345.775950	52.491796	66.876404
1345.030026	49.633257	66.881409
1344.765962	46.370117	66.886414
1344.492994	41.099408	66.891418
1343.057301	53.630806	66.896423
1342.965629	44.589261	66.901428
1342.076809	45.005033	66.906433
1341.516056	41.205605	66.911438
1340.876379	39.825090	66.916442
1339.790855	54.991033	66.921447
1339.618284	43.920248	66.926452
1338.820432	51.600586	66.931457
1338.170867	44.763951	66.936462
1337.453213	42.528532	66.941466
1336.677290	46.138528	66.946471
1336.487476	41.362366	66.951476
1335.496754	38.782441	66.956481
1334.624536	39.533036	66.961486
1334.123121	46.297367	66.966490
1333.521417	56.242509	66.971495
1333.086113	38.472197	66.976500
1332.129351	43.364587	66.981505
1331.473666	50.186562	66.986510
1331.038218	37.604317	66.991514
1329.913146	50.819599	66.996519
1329.254629	34.672730	67.001524
1328.611013	51.124560	67.006529
1327.913652	44.252950	67.011534
1328.083775	29.087649	67.016538
1326.955963	51.449449	67.021543
1326.278518	30.532283	67.026548
1325.556558	36.155298	67.031553
1325.042511	43.512979	67.036558
1324.570391	43.755280	67.041562
1323.328631	43.553829	67.046567
1323.410124	32.499432	67.051572
1322.382267	46.656442	67.056577
1321.109315	41.680333	67.061582
1320.771207	35.383956	67.066586
1319.958701	40.016877	67.071591
1319.752021	39.138371	67.076596
1319.368877	42.198658	67.081601
1318.595767	38.600150	67.086606
1317.809537	38.151243	67.091610
1317.234119	41.846057	67.096615
1316.405149	33.647121	67.101620
1315.344586	39.174167	67.106625
1314.780377	41.395941	67.111630
1314.793962	33.435202	67.116634
1313.341094	38.365471	67.121639
1312.672791	37.169284	67.126644
1311.882065	46.062714	67.131649
1311.650355	34.782153	67.136654
1311.445075	42.956468	67.141658
1310.631654	43.481686	67.146663
1309.997434	32.809156	67.151668
1309.186482	34.565548	67.156673
1308.601664	38.921006	67.161678
1307.605908	36.833889	67.166682
1306.777070	43.397973	67.171687
1306.417166	36.092687	67.176692
1305.924351	40.517094	67.181697
1304.930230	51.477082	67.186702
1304.414579	46.505152	67.191706
1303.627535	48.651975	67.196711
1303.384001	47.251063	67.201716
1303.029872	37.406032	67.206721
1301.694348	44.459097	67.211726
1301.348179	44.250879	67.216730
1300.362791	48.225340	67.221735
1299.713654	35.437391	67.226740
1298.805512	42.621196	67.231745
1297.996368	38.637350	67.236750
1298.156652	36.468934	67.241754
1297.374494	50.478082	67.246759
1296.549788	34.141614	67.251764
1295.646654	33.768070	67.256769
1295.117590	36.157719	67.261774
1295.207139	45.720148	67.266778
1293.565630	46.753915	67.271783
1293.213608	33.135006	67.276788
1292.759798	33.686629	67.281793
1291.853829	44.463870	67.286798
1290.971806	30.741579	67.291802
1289.845332	37.275720	67.296807
1289.721377	40.641721	67.301812
1289.298075	41.464453	67.306817
1288.968706	42.497749	67.311822
1288.476464	44.288628	67.316826
1287.101566	33.129915	67.321831
1286.542593	37.508074	67.326836
1286.164795	29.510223	67.331841
1284.969636	32.967697	67.336846
1284.238136	34.780848	67.341850
1283.648348	38.151531	67.346855
1283.722596	21.311040	67.351860
1283.093310	37.434158	67.356865
1281.765147	48.497723	67.361870
1281.500777	25.433385	67.366874
1281.061580	34.885916	67.371879
1280.151803	25.521897	67.376884
1278.994253	40.237258	67.381889
1278.469562	35.478083	67.386894
1278.366135	23.868066	67.391898
1277.326197	33.286808	67.396903
1276.268447	33.146007	67.401908
1276.011627	27.782863	67.406913
1275.422211	37.457971	67.411918
1275.181236	35.973081	67.416922
1273.875168	40.318649	67.421927
1273.095035	31.017593	67.426932
1272.706445	35.709274	67.431937
1272.388511	32.487829	67.436942
1271.982935	35.655763	67.441946
1270.835969	34.437928	67.446951
1270.490907	22.136226	67.451956
1269.161427	32.280656	67.456961
1268.462666	38.521298	67.461966
1268.421359	32.559353	67.466970
1267.558628	44.361022	67.471975
1266.854613	36.269967	67.476980
1266.223100	39.773442	67.481985
1265.485294	46.334101	67.486990
1265.209432	45.070795	67.491994
1263.971660	37.777375	67.496999
1263.102977	29.520125	67.502004
1262.510892	46.419486	67.507009
1262.468922	40.225838	67.512014
1262.008679	36.427795	67.517018
1260.765025	41.807360	67.522023
1260.250355	44.276728	67.527028
1259.567892	35.185642	67.532033
1258.272968	41.456429	67.537038
1257.889984	38.956514	67.542042
1257.261092	49.082598	67.547047
1256.832646	41.122763	67.552052
1256.653076	38.342929	67.557057
1255.751502	40.339246	67.562062
1254.973746	36.886575	67.567066
1254.250162	40.576575	67.572071
1254.139935	36.200921	67.577076
1252.812796	36.221233	67.582081
1252.237197	31.925888	67.587086
1251.935485	31.456726	67.592090
1250.814547	41.856583	67.597095
1250.138737	41.341254	67.602100
1249.452200	43.456341	67.607105
1248.885386	35.785011	67.612110
1248.489176	31.060606	67.617114
1247.543524	39.210726	67.622119
1246.948013	41.576259	67.627124
1246.065804	40.966022	67.632129
1245.881048	46.066832	67.637134
1245.485481	28.610359	67.642138
1243.789405	32.063926	67.647143
1243.680870	37.527917	67.652148
1243.232019	28.954766	67.657153
1242.528327	37.290332	67.662158
1241.815146	39.564193	67.667162
1240.943280	54.926414	67.672167
1240.633994	41.191911	67.677172
1239.730162	42.431675	67.682177
1238.680938	45.916427	67.687182
1238.452666	46.345465	67.692186
1237.873119	52.458356	67.697191
1237.148504	44.838925	67.702196
1236.231423	36.452188	67.707201
1235.387366	35.749158	67.712206
1235.307413	46.234218	67.717210
1234.515718	45.494477	67.722215
1233.832308	25.644304	67.727220
1233.030521	38.349314	67.732225
1232.195371	40.286192	67.737230
1232.319725	32.976455	67.742234
1231.091418	48.958310	67.747239
1230.512840	38.784721	67.752244
1229.877206	34.536773	67.757249
1229.103607	38.017119	67.762254
1228.435633	31.986100	67.767258
1227.467975	47.051321	67.772263
1227.400152	39.163455	67.777268
1227.113342	43.452615	67.782273
1225.975708	51.579662	67.787278
1225.569176	35.962032	67.792282
1224.339336	46.924830	67.797287
1223.300429	39.290733	67.802292
1222.848773	42.502272	67.807297
1222.167021	41.909050	67.812302
1221.930167	36.180048	67.817306
1221.430172	44.506883	67.822311
1221.122357	40.380265	67.827316
1220.029951	33.940516	67.832321
1219.349073	46.290427	67.837326
1218.702753	42.208178	67.842330
1217.701709	34.872409	67.847335
1217.355852	41.326594	67.852340
1216.981437	45.836263	67.857345
1215.494315	49.720235	67.862350
1215.031031	35.904580	67.867354
1214.263810	41.615242	67.872359
1213.715624	41.243626	67.877364
1213.191854	41.043164	67.882369
1212.685369	40.049923	67.887374
1212.857176	32.041955	67.892378
1211.527839	47.762345	67.897383
1210.733119	36.328494	67.902388
1209.868444	39.231988	67.907393
1208.735719	38.278414	67.912398
1208.417971	29.427387	67.917402
1207.796275	43.854134	67.922407
1207.803538	47.320692	67.927412
1207.027269	38.932074	67.932417
1206.072152	37.697951	67.937422
1205.651637	30.351869	67.942426
1204.203219	43.904023	67.947431
1203.333966	32.748529	67.952436
1203.161713	40.666861	67.957441
1202.593394	47.952768	67.962446
1202.543281	41.739918	67.967450
1201.972983	34.687306	67.972455
1200.961733	37.428037	67.977460
1200.321065	31.726990	67.982465
1199.474585	39.984351	67.987470
1198.483273	40.411742	67.992474
1197.579756	43.450724	67.997479
1197.716033	31.034640	68.002484
1197.471456	33.975135	68.007489
1196.424788	42.125566	68.012494
1195.473393	30.410723	68.017498
1194.550786	44.445370	68.022503
1194.036070	38.688023	68.027508
1193.132792	42.028158	68.032513
1192.400306	42.357620	68.037518
1192.094380	28.037574	68.042522
1191.659837	41.392221	68.047527
1191.408159	41.485951	68.052532
1190.403205	36.043106	68.057537
1189.685178	41.734913	68.062542
1189.094368	36.738701	68.067546
1187.683381	40.282580	68.072551
1187.150687	33.938331	68.077556
1186.997218	42.528594	68.082561
1186.563013	43.010887	68.087566
1185.905293	37.859742	68.092570
1185.006948	35.664146	68.097575
1184.869687	43.851297	68.102580
1183.466940	37.453036	68.107585
1182.730875	43.903052	68.112590
1181.987017	45.448546	68.117594
1181.229805	38.129206	68.122599
1181.284154	35.887749	68.127604
1180.389538	42.331443	68.132609
1179.237801	38.353242	68.137614
1178.808789	46.484295	68.142618
1178.360913	48.523597	68.147623
1177.718052	45.684990	68.152628
1176.738320	42.426889	68.157633
1176.135204	44.396265	68.162638
1175.827368	36.122390	68.167642
1175.118293	43.845411	68.172647
1174.409759	42.084819	68.177652
1173.854306	31.294159	68.182657
1173.051425	49.277274	68.187662
1172.355012	37.217540	68.192666
1171.339446	45.588533	68.197671
1170.436532	45.508303	68.202676
1170.131074	39.842256	68.207681
1169.922167	43.299038	68.212686
1169.573808	42.578692	68.217690
1168.178676	45.312684	68.222695
1167.483573	36.878058	68.227700
1167.648710	35.796932	68.232705
1166.591613	43.375038	68.237710
1166.035074	37.373622	68.242714
1165.353569	36.832414	68.247719
1164.615195	31.449685	68.252724
1163.550114	44.967696	68.257729
1163.072938	44.422376	68.262734
1162.828648	38.353952	68.267738
1161.984423	42.304430	68.272743
1160.787956	45.041520	68.277748
1160.312765	50.169603	68.282753
1159.820342	41.787895	68.287758
1159.264729	41.236128	68.292762
1158.374706	35.363446	68.297767
1157.740462	41.899771	68.302772
1157.633159	38.167039	68.307777
1156.266140	39.969343	68.312782
1155.630594	34.873026	68.317786
1155.231562	38.550853	68.322791
1154.726294	52.754098	68.327796
1153.829282	38.944369	68.332801
1152.713444	42.201633	68.337806
1152.542395	33.530704	68.342810
1152.053397	35.477203	68.347815
1151.667389	42.343044	68.352820
1150.457101	41.393949	68.357825
1149.588726	49.858231	68.362830
1149.214131	38.204624	68.367834
1148.746030	37.604249	68.372839
1147.588080	39.109961	68.377844
1146.931743	32.766467	68.382849
1146.346951	46.170247	68.387854
1146.164132	29.343848	68.392858
1145.833472	40.280344	68.397863
1144.485257	41.007365	68.402868
1144.062449	29.996929	68.407873
1143.487756	44.832511	68.412878
1142.981886	32.774025	68.417882
1142.198213	35.543233	68.422887
1141.361294	25.519581	68.427892
1140.540517	26.333019	68.432897
1139.678656	44.211975	68.437902
1139.134035	36.414149	68.442906
1138.568784	30.784703	68.447911
1138.321630	30.980217	68.452916
1137.591573	39.834068	68.457921
1136.386533	36.692244	68.462926
1136.262052	29.920394	68.467930
1135.584526	26.669437	68.472935
1134.282370	38.853251	68.477940
1133.998557	40.131624	68.482945
1133.208304	34.378698	68.487950
1132.970617	29.529759	68.492954
1132.396252	38.984879	68.497959
1131.314693	30.804122	68.502964
1130.724111	45.033546	68.507969
1130.224380	43.553559	68.512974
1129.508080	39.056704	68.517978
1128.778202	45.852668	68.522983
1128.098301	40.687722	68.527988
1127.676636	31.736549	68.532993
1126.469912	44.275764	68.537998
1125.878066	29.504488	68.543002
1125.324728	41.807313	68.548007
1124.971234	33.564366	68.553012
1124.476737	35.946971	68.558017
1123.394369	40.845214	68.563022
1122.839111	44.312937	68.568026
1122.144933	30.494622	68.573031
1121.408277	31.528067	68.578036
1120.694255	37.266557	68.583041
1120.199735	39.707513	68.588046
1119.828156	29.177777	68.593050
1118.739103	33.119900	68.598055
1117.645168	41.996945	68.603060
1117.419192	38.013441	68.608065
1116.984640	35.641600	68.613070
1116.527445	37.870044	68.618074
1115.454180	22.883628	68.623079
1114.900649	41.110919	68.628084
1114.187991	38.026399	68.633089
1113.724822	40.038181	68.638094
1113.235982	35.766918	68.643098
1112.178077	36.536084	68.648103
1111.695256	31.199453	68.653108
1110.877792	37.164128	68.658113
1109.831626	36.884362	68.663118
1109.646050	35.455331	68.668122
1108.981554	39.894460	68.673127
1108.256355	34.815573	68.678132
1107.375951	30.964555	68.683137
1106.415192	31.904347	68.688142
1106.179715	26.253992	68.693146
1105.810566	39.951465	68.698151
1105.407909	36.342987	68.703156
1104.575869	26.698609	68.708161
1103.725892	36.810989	68.713166
1103.305525	30.341668	68.718170
1102.342625	24.666682	68.723175
1101.616368	31.764835	68.728180
1101.433602	24.237464	68.733185
1100.547900	32.193587	68.738190
1099.365749	34.472700	68.743194
1099.007668	30.808250	68.748199
1098.521878	43.037257	68.753204
1098.358378	26.128956	68.758209
1097.199412	38.482388	68.763214
1096.466182	31.433651	68.768218
1095.284907	33.676357	68.773223
1094.268986	26.737244	68.778228
1094.087582	36.964040	68.783233
1093.340332	35.094518	68.788238
1093.389058	28.946383	68.793242
1093.020271	32.863825	68.798247
1092.110735	34.934000	68.803252
1091.642834	28.139517	68.808257
1090.597457	34.932057	68.813262
1089.890647	34.935775	68.818266
1089.229729	34.099587	68.823271
1088.460524	39.544096	68.828276
1087.991659	29.897143	68.833281
1086.667414	40.960157	68.838286
1086.353265	33.898370	68.843290
1085.561337	36.052338	68.848295
1085.122858	46.591264	68.853300
1084.885739	24.921380	68.858305
1083.581620	38.948927	68.863310
1083.043002	31.060283	68.868314
1082.619266	26.080105	68.873319
1081.429638	34.972380	68.878324
1081.505392	44.172706	68.883329
1080.363695	41.094948	68.888334
1079.788429	38.015390	68.893338
1079.406579	41.980644	68.898343
1078.763947	34.551657	68.903348
1077.880869	26.996925	68.908353
1077.306574	37.311453	68.913358
1077.001777	40.245768	68.918362
1075.764006	41.100331	68.923367
1074.889376	36.243917	68.928372
1074.540700	35.752287	68.933377
1074.180163	43.333152	68.938382
1073.678221	43.660665	68.943386
1072.608006	38.795941	68.948391
1071.931265	41.641197	68.953396
1071.554302	42.566976	68.958401
1070.205933	40.304246	68.963406
1069.646029	30.100940	68.968410
1069.216296	44.787313	68.973415
1068.812076	30.719473	68.978420
1068.350971	36.021935	68.983425
1067.354203	37.491002	68.988430
1066.300707	36.449198	68.993434
1065.960837	36.878659	68.998439
1065.411020	33.690981	69.003444
1064.723779	39.507222	69.008449
1064.127418	48.691474	69.013454
1063.305613	41.863409	69.018458
1062.889898	37.815484	69.023463
1061.507082	40.856644	69.028468
1061.388491	37.021640	69.033473
1060.451147	51.848696	69.038478
1060.173804	29.945523	69.043482
1059.376821	38.131966	69.048487
1058.521260	38.567776	69.053492
1057.996915	43.850342	69.058497
1057.509732	37.990882	69.063502
1057.209720	30.647743	69.068506
1056.102044	36.958212	69.073511
1055.395857	45.568596	69.078516
1055.703657	30.425572	69.083521
1054.295883	49.119924	69.088526
1053.534198	36.045635	69.093530
1052.977176	35.189774	69.098535
1051.821812	34.623062	69.103540
1051.313463	28.697591	69.108545
1050.375505	35.897244	69.113550
1050.083413	43.180224	69.118554
1049.835779	33.827657	69.123559
1048.830831	42.946026	69.128564
1048.348351	30.011824	69.133569
1047.283917	37.103870	69.138574
1047.085259	33.973868	69.143578
1046.263199	33.256365	69.148583
1045.139265	42.683815	69.153588
1045.254220	38.232933	69.158593
1044.655451	31.399358	69.163598
1043.651743	25.087513	69.168602
1042.832721	40.829264	69.173607
1042.151194	44.963622	69.178612
1042.026118	28.713097	69.183617
1040.682104	36.376310	69.188622
1040.195394	32.987793	69.193626
1039.703649	39.704889	69.198631
1038.442527	31.915435	69.203636
1037.913932	28.289164	69.208641
1037.487316	43.350343	69.213646
1037.160291	39.889113	69.218650
1036.688124	39.227906	69.223655
1035.564998	44.455933	69.228660
1035.253638	29.020346	69.233665
1034.547396	45.299231	69.238670
1033.776059	26.604825	69.243674
1032.681261	37.814274	69.248679
1031.806905	41.003206	69.253684
1032.029111	24.957625	69.258689
1031.574702	33.911137	69.263694
1030.351627	38.481727	69.268698
1029.739968	35.196668	69.273703
1029.054800	46.183262	69.278708
1028.199570	28.468847	69.283713
1027.135369	37.301766	69.288718
1026.614410	30.831121	69.293722
1026.343237	34.944345	69.298727
1026.271225	35.422655	69.303732
1025.620419	21.586451	69.308737
1024.496941	48.515906	69.313742
1023.815674	31.984875	69.318746
1022.841419	28.286014	69.323751
1021.738831	47.100548	69.328756
1021.672001	39.731349	69.333761
1020.840045	38.777316	69.338766
1020.740017	37.796715	69.343770
1020.399631	28.047343	69.348775
1019.321611	30.694687	69.353780
1018.785438	36.807013	69.358785
1017.621899	44.736408	69.363790
1016.788761	31.386511	69.368794
1016.222612	37.784296	69.373799
1015.536814	29.417635	69.378804
1015.826611	28.433358	69.383809
1014.828898	30.058708	69.388814
1014.185774	39.919009	69.393818
1013.554022	29.462233	69.398823
1012.245332	31.649557	69.403828
1011.706246	29.229716	69.408833
1010.726499	27.181176	69.413838
1010.472123	31.249151	69.418842
1010.118052	39.180638	69.423847
1008.725906	36.139609	69.428852
1008.424351	35.011307	69.433857
1008.159117	33.271694	69.438862
1007.805189	29.247066	69.443866
1006.637574	31.123372	69.448871
1005.835850	46.964883	69.453876
1005.467679	31.133076	69.458881
1004.429733	40.649357	69.463886
1003.644925	36.444134	69.468890
1003.210896	44.962340	69.473895
1002.594457	48.485550	69.478900
1002.341158	34.247062	69.483905
1001.061698	46.110363	69.488910
1000.255317	36.898744	69.493914
1000.104733	43.279297	69.498919
999.664376	28.627468	69.503924
998.617819	32.704797	69.508929
997.929072	32.653629	69.513934
997.745141	32.055375	69.518938
996.678509	31.942911	69.523943
995.596041	35.429887	69.528948
995.222869	32.166814	69.533953
994.646535	34.343272	69.538958
994.418147	37.418396	69.543962
993.234243	40.033716	69.548967
992.782498	43.907602	69.553972
992.376698	36.294307	69.558977
991.255772	36.887477	69.563982
990.653329	29.797469	69.568986
989.778916	37.808596	69.573991
989.400879	41.940405	69.578996
989.111825	33.065936	69.584001
987.904171	36.490834	69.589006
987.441119	45.773728	69.594010
986.901318	45.205292	69.599015
986.027834	38.241984	69.604020
985.151774	29.624918	69.609025
984.258330	30.661273	69.614030
983.883613	44.007984	69.619034
983.665323	43.558697	69.624039
983.311164	46.781565	69.629044
982.642710	36.504095	69.634049
981.619011	38.299169	69.639054
980.893889	35.369634	69.644058
979.501831	48.725268	69.649063
979.022149	44.913033	69.654068
978.637360	29.642106	69.659073
978.065692	34.747712	69.664078
977.787110	38.485239	69.669082
976.834325	34.905978	69.674087
975.850982	38.068116	69.679092
975.700559	25.697675	69.684097
975.228452	33.923901	69.689102
974.588067	33.732584	69.694106
973.628525	39.190062	69.699111
972.739204	50.168153	69.704116
972.563201	39.465407	69.709121
971.104930	42.602197	69.714126
970.972354	48.949926	69.719130
970.534462	26.998221	69.724135
969.959859	31.656454	69.729140
968.701359	37.568345	69.734145
968.275862	38.889779	69.739150
967.414023	46.613497	69.744154
966.735102	36.858077	69.749159
965.855567	43.588006	69.754164
965.392301	39.088787	69.759169
964.902964	48.744863	69.764174
964.693218	42.814471	69.769178
964.128599	42.893366	69.774183
962.957266	45.405778	69.779188
962.506336	37.686134	69.784193
961.332778	46.064986	69.789198
960.648241	37.447412	69.794202
960.061886	50.081930	69.799207
959.616062	48.859898	69.804212
959.450108	43.357765	69.809217
958.687934	40.490901	69.814222
957.996398	50.533957	69.819226
957.415267	39.816835	69.824231
955.973435	43.636971	69.829236
955.189528	57.037769	69.834241
954.657374	50.021731	69.839246
954.338747	42.795105	69.844250
954.144677	42.195314	69.849255
953.379179	43.173475	69.854260
952.454514	49.793900	69.859265
951.916976	42.915914	69.864270
951.056654	42.933060	69.869274
949.905394	44.258028	69.874279
949.264738	50.839568	69.879284
949.151861	34.170814	69.884289
948.700406	46.479521	69.889294
948.094347	50.720159	69.894298
947.302251	34.561601	69.899303
946.509393	52.327114	69.904308
945.913860	41.870899	69.909313
945.242237	44.094070	69.914318
944.323610	44.740221	69.919322
943.743012	36.394686	69.924327
943.287464	52.460236	69.929332
942.527647	28.851980	69.934337
941.347552	46.158731	69.939342
940.930538	45.264845	69.944346
940.830068	40.715783	69.949351
940.322634	40.837622	69.954356
939.365848	40.010710	69.959361
938.427252	47.484883	69.964366
938.051411	44.796236	69.969370
936.783769	37.190798	69.974375
935.782221	52.304056	69.979380
935.785561	40.672363	69.984385
935.130440	30.329718	69.989390
935.162530	38.183987	69.994394
934.522843	36.603317	69.999399
933.119578	44.783775	70.004404
932.872104	35.521088	70.009409
931.980929	36.112413	70.014414
930.944492	36.769432	70.019418
930.990161	28.991274	70.024423
929.892369	37.946260	70.029428
929.505623	40.690209	70.034433
928.393872	45.471780	70.039438
927.833233	36.657888	70.044442
927.594461	35.238916	70.049447
926.588324	46.899482	70.054452
926.080323	36.216466	70.059457
925.492628	42.452121	70.064462
924.823279	40.146066	70.069466
924.092274	39.792570	70.074471
923.169247	46.086322	70.079476
922.745188	30.611933	70.084481
922.302600	38.887084	70.089486
921.300921	27.782761	70.094490
920.819736	28.414496	70.099495
920.002419	40.825577	70.104500
919.189169	31.630858	70.109505
918.265888	47.630494	70.114510
917.727481	37.332352	70.119514
917.498900	36.567751	70.124519
916.899477	34.055036	70.129524
916.496115	27.422211	70.134529
915.119456	41.305252	70.139534
914.338258	42.301691	70.144538
913.990233	46.390887	70.149543
913.662639	38.683166	70.154548
913.045609	43.715584	70.159553
912.068578	36.156949	70.164558
911.606942	37.501489	70.169562
911.007400	42.006015	70.174567
909.746346	39.016719	70.179572
909.307653	35.891817	70.184577
908.708118	42.873658	70.189582
908.354484	43.122409	70.194586
908.001991	41.645845	70.199591
906.768076	46.399560	70.204596
906.585235	41.247041	70.209601
905.511004	43.844946	70.214606
904.485732	43.339597	70.219610
904.196668	37.849181	70.224615
903.319087	42.227652	70.229620
903.261081	34.562184	70.234625
902.087719	40.324941	70.239630
901.193154	37.707818	70.244634
901.004312	37.334274	70.249639
900.423055	42.630651	70.254644
899.539494	41.276454	70.259649
898.779310	38.376179	70.264654
898.074124	42.370834	70.269658
897.918045	33.763795	70.274663
897.038548	41.108727	70.279668
896.201278	28.970610	70.284673
895.468300	40.491514	70.289678
895.159685	36.227889	70.294682
894.241124	36.052481	70.299687
893.364672	43.761195	70.304692
893.159788	37.432663	70.309697
892.816318	31.613453	70.314702
891.690220	38.813135	70.319706
891.009199	26.022548	70.324711
890.256484	43.392173	70.329716
889.676303	41.565508	70.334721
888.810177	33.673854	70.339726
888.223193	43.400665	70.344730
887.829058	32.187048	70.349735
887.102104	35.265835	70.354740
886.242134	31.665534	70.359745
885.838985	40.913668	70.364750
885.547247	35.828946	70.369754
884.590001	31.342138	70.374759
883.304704	37.035988	70.379764
883.002872	36.749812	70.384769
882.505313	26.560302	70.389774
881.744972	38.254291	70.394778
880.632477	33.632926	70.399783
880.007236	34.650284	70.404788
879.651119	31.362442	70.409793
879.513154	33.650498	70.414798
878.939162	47.848918	70.419802
878.211337	33.165610	70.424807
877.144695	44.993508	70.429812
876.150995	45.785668	70.434817
875.393591	38.255170	70.439822
874.942264	39.615422	70.444826
874.714222	37.526140	70.449831
873.827521	44.273004	70.454836
872.981121	31.978657	70.459841
872.408320	44.413909	70.464846
871.892635	36.417600	70.469850
871.585273	39.606223	70.474855
870.311016	41.114799	70.479860
869.743965	34.970067	70.484865
869.193748	44.096537	70.489870
868.616446	34.955744	70.494874
867.661837	36.541175	70.499879
866.800997	49.273004	70.504884
866.704414	34.596458	70.509889
866.314235	40.961529	70.514894
865.469449	42.972592	70.519898
864.697271	35.061263	70.524903
864.024209	51.192970	70.529908
863.426396	41.038336	70.534913
862.325881	36.410342	70.539918
861.759048	42.339921	70.544922
861.553902	37.717645	70.549927
860.465550	43.101049	70.554932
859.779771	34.053216	70.559937
859.220237	46.237208	70.564942
858.539030	32.743359	70.569946
858.452048	43.067081	70.574951
857.146712	41.196578	70.579956
856.656286	31.466393	70.584961
855.892137	49.765068	70.589966
855.419886	33.506763	70.594970
854.367364	40.270562	70.599975
853.902272	39.119425	70.604980
853.503947	40.584781	70.609985
853.100497	48.582487	70.614990
852.059947	42.175665	70.619994
851.651196	37.208918	70.624999
850.437680	47.040192	70.630004
850.180079	32.971158	70.635009
849.038100	43.148999	70.640014
848.344058	35.591082	70.645018
847.800265	40.056784	70.650023
847.498455	46.034067	70.655028
847.174211	41.528517	70.660033
846.246864	34.155965	70.665038
845.553516	36.686959	70.670042
845.067371	34.123117	70.675047
844.301835	38.561039	70.680052
843.746080	26.586290	70.685057
842.802310	35.485251	70.690062
841.607026	44.988782	70.695066
841.254790	32.267298	70.700071
840.646478	48.059124	70.705076
840.634843	31.945122	70.710081
839.705233	41.657091	70.715086
838.635720	34.819665	70.720090
838.096895	37.994672	70.725095
837.420333	39.860698	70.730100
836.862166	36.524601	70.735105
836.381360	38.272738	70.740110
835.805742	36.677166	70.745114
835.208896	36.366994	70.750119
834.004960	36.845716	70.755124
833.483695	30.734708	70.760129
832.991976	40.389592	70.765134
832.094407	43.632743	70.770138
831.516607	33.019215	70.775143
830.635119	39.088768	70.780148
830.161619	38.446737	70.785153
829.704338	44.114464	70.790158
828.610940	36.530238	70.795162
828.212873	38.952736	70.800167
826.869132	38.895492	70.805172
827.126193	36.877227	70.810177
826.968051	41.406121	70.815182
825.643588	40.568397	70.820186
825.562265	34.934545	70.825191
823.981058	34.039922	70.830196
823.438111	34.900695	70.835201
822.689957	36.655122	70.840206
822.196107	39.715744	70.845210
821.834073	36.979192	70.850215
820.603882	44.069320	70.855220
820.094914	32.992268	70.860225
819.363611	25.299954	70.865230
819.028606	39.673210	70.870234
818.967411	35.663517	70.875239
817.458628	37.546909	70.880244
817.141637	30.808896	70.885249
816.745904	37.157508	70.890254
815.445834	43.974919	70.895258
814.810395	36.816102	70.900263
814.009767	35.398274	70.905268
813.483028	31.522612	70.910273
813.471532	34.966907	70.915278
812.387588	42.899476	70.920282
811.886208	42.605651	70.925287
811.178867	45.607223	70.930292
810.403117	31.229611	70.935297
809.495601	37.421580	70.940302
809.097918	51.697595	70.945306
808.633815	40.637054	70.950311
807.693865	47.822908	70.955316
806.776943	36.183192	70.960321
806.557861	30.574427	70.965326
805.852889	44.848891	70.970330
805.392564	35.492385	70.975335
804.532820	37.278773	70.980340
803.636293	37.993993	70.985345
803.448485	36.879148	70.990350
802.533943	32.790841	70.995354
802.104060	31.667225	71.000359
801.318018	39.137649	71.005364
800.533329	30.980767	71.010369
799.871481	36.772520	71.015374
798.841659	44.373214	71.020378
798.359825	25.654921	71.025383
798.074290	34.307188	71.030388
797.035313	44.686264	71.035393
796.292377	42.461345	71.040398
795.712420	35.350471	71.045402
795.701939	32.318271	71.050407
794.530732	44.251145	71.055412
793.842386	33.429731	71.060417
793.039307	42.088700	71.065422
792.716113	43.602027	71.070426
792.240449	39.030709	71.075431
790.809342	40.990057	71.080436
790.377649	22.907164	71.085441
790.147365	40.486933	71.090446
789.367510	33.748495	71.095450
788.661211	35.351194	71.100455
787.946430	31.286284	71.105460
787.547980	28.296925	71.110465
786.633196	29.678932	71.115470
785.815610	30.747432	71.120474
785.501433	33.441999	71.125479
784.891004	30.587307	71.130484
783.964584	28.636024	71.135489
783.306608	29.917227	71.140494
782.631405	47.427488	71.145498
782.200980	31.168863	71.150503
781.042077	40.687121	71.155508
780.337760	38.118603	71.160513
779.824240	26.763183	71.165518
779.104615	36.284046	71.170522
779.364048	21.891465	71.175527
777.831583	36.866921	71.180532
777.445842	39.361577	71.185537
776.959207	32.973844	71.190542
775.805096	31.596534	71.195546
775.418386	24.456485	71.200551
774.615207	37.134988	71.205556
774.040535	36.975837	71.210561
773.878532	32.632125	71.215566
772.497333	37.054541	71.220570
772.131178	24.713755	71.225575
771.571987	25.807353	71.230580
770.910334	25.345093	71.235585
770.106107	34.713851	71.240590
769.274495	41.133438	71.245594
769.588038	17.575184	71.250599
767.989970	38.282080	71.255604
767.130014	40.749735	71.260609
766.561085	24.528942	71.265614
766.204196	30.273726	71.270618
765.642918	27.160488	71.275623
764.643174	30.326887	71.280628
763.869403	38.052400	71.285633
763.742669	28.439381	71.290638
763.168318	34.037444	71.295642
762.207262	25.528626	71.300647
761.256771	34.357718	71.305652
760.836872	33.120560	71.310657
760.671658	32.431039	71.315662
759.604215	32.052309	71.320666
758.891719	35.871547	71.325671
758.371985	29.118518	71.330676
757.917618	28.268459	71.335681
757.052993	32.968173	71.340686
756.209226	33.235054	71.345690
755.659819	29.482861	71.350695
754.518112	39.216003	71.355700
753.799674	28.623320	71.360705
753.438343	39.914773	71.365710
752.933751	34.942807	71.370714
752.607152	45.463939	71.375719
751.573624	41.941779	71.380724
750.739472	38.802602	71.385729
750.722608	33.103304	71.390734
749.752955	43.927081	71.395738
748.929531	36.895983	71.400743
748.161253	40.139075	71.405748
747.859773	36.073029	71.410753
747.045416	32.604286	71.415758
745.938595	40.204639	71.420762
745.930273	27.735927	71.425767
745.152626	32.855444	71.430772
744.596673	39.089227	71.435777
743.713635	34.784624	71.440782
742.742453	33.188977	71.445786
742.635138	37.389668	71.450791
741.421885	38.421833	71.455796
740.457673	33.698084	71.460801
740.654946	30.672232	71.465806
739.811476	36.816178	71.470810
739.370818	42.446577	71.475815
738.240739	33.535759	71.480820
737.696976	38.624350	71.485825
737.576927	20.155983	71.490830
736.050633	36.373070	71.495834
735.489706	37.854870	71.500839
735.139000	38.059025	71.505844
734.559343	30.894510	71.510849
734.044424	26.865605	71.515854
733.029736	25.872958	71.520858
732.792283	28.533237	71.525863
732.099771	30.679362	71.530868
730.964515	43.283022	71.535873
730.139950	29.515598	71.540878
729.525703	29.123070	71.545882
729.495527	33.724626	71.550887
728.720300	36.554105	71.555892
727.769757	29.771909	71.560897
727.281005	26.866322	71.565902
726.617626	39.222967	71.570906
725.833269	32.460041	71.575911
725.113828	38.432862	71.580916
724.319820	35.197421	71.585921
724.313717	21.838992	71.590926
722.871308	45.717506	71.595930
722.147440	31.267022	71.600935
721.863269	28.218480	71.605940
721.243353	32.770436	71.610945
720.951187	25.793535	71.615950
719.704328	31.139148	71.620954
719.705858	24.730476	71.625959
718.768457	45.034175	71.630964
717.986844	42.821747	71.635969
717.445836	33.985875	71.640974
716.386943	38.450039	71.645978
716.356009	26.924764	71.650983
715.179120	42.334053	71.655988
714.347648	29.305726	71.660993
714.058605	28.727386	71.665998
713.425860	30.556504	71.671002
712.889881	37.578714	71.676007
711.678175	40.375198	71.681012
711.387139	40.356974	71.686017
710.877164	25.268492	71.691022
709.468848	33.495582	71.696026
708.992724	31.305478	71.701031
708.690882	26.687584	71.706036
708.054551	30.286554	71.711041
707.866357	29.958653	71.716046
706.472455	42.310199	71.721050
705.891687	33.316665	71.726055
705.519437	45.298967	71.731060
704.803685	42.144108	71.736065
704.005759	28.984293	71.741070
702.980376	50.710182	71.746074
702.837251	43.810466	71.751079
702.043989	35.941982	71.756084
701.598673	34.007161	71.761089
700.818188	35.173856	71.766094
700.037203	43.275837	71.771098
699.903085	40.011021	71.776103
698.510057	40.056308	71.781108
697.721058	38.109983	71.786113
697.678050	33.780447	71.791118
697.340021	30.967557	71.796122
696.200049	35.116643	71.801127
695.700152	33.229937	71.806132
694.902785	34.113903	71.811137
694.003594	36.267718	71.816142
692.862490	36.004821	71.821146
692.665807	31.294493	71.826151
692.162332	26.211985	71.831156
691.484510	39.733108	71.836161
691.365303	41.035775	71.841166
689.915926	41.449573	71.846170
689.606285	38.843468	71.851175
689.023405	36.862748	71.856180
688.016452	48.110362	71.861185
687.329690	38.189145	71.866190
686.575487	35.445679	71.871194
686.637204	37.793405	71.876199
686.010516	30.641126	71.881204
685.235095	40.314390	71.886209
685.080378	26.328368	71.891214
683.465188	34.998407	71.896218
682.687711	24.364696	71.901223
681.805292	39.481105	71.906228
681.596938	27.802743	71.911233
681.181274	29.163655	71.916238
679.616093	37.399971	71.921242
679.387702	26.472251	71.926247
678.889896	36.318920	71.931252
678.658758	36.959767	71.936257
677.645822	32.712144	71.941262
676.764266	31.764550	71.946266
676.398394	25.565767	71.951271
675.745513	29.794986	71.956276
675.177662	28.576673	71.961281
674.642097	29.031039	71.966286
674.008896	34.299455	71.971290
672.972292	27.718641	71.976295
672.324386	28.135705	71.981300
671.338087	29.251606	71.986305
671.342839	27.833307	71.991310
670.386756	30.060841	71.996314
669.673290	28.660721	72.001319
669.101069	25.467252	72.006324
668.643569	31.054607	72.011329
667.540054	33.384465	72.016334
666.738466	32.280643	72.021338
666.247573	32.956547	72.026343
666.291858	28.392348	72.031348
665.107805	35.574534	72.036353
664.435267	30.189382	72.041358
663.809176	34.627219	72.046362
663.212593	26.437287	72.051367
662.467407	33.677314	72.056372
661.266438	46.802379	72.061377
660.932738	31.401996	72.066382
660.121960	36.880037	72.071386
659.953224	35.547709	72.076391
659.502846	34.091504	72.081396
658.382287	35.217753	72.086401
658.326361	23.341667	72.091406
657.321809	34.997313	72.096410
656.602400	30.370232	72.101415
655.869964	35.618186	72.106420
655.361107	37.667279	72.111425
654.876414	37.648363	72.116430
654.003015	49.240559	72.121434
653.343861	29.829914	72.126439
652.332320	32.394281	72.131444
651.035223	33.401995	72.136449
650.742327	30.233432	72.141454
650.623852	39.116134	72.146458
649.991118	36.446374	72.151463
649.606281	40.591916	72.156468
648.622959	32.515610	72.161473
648.156957	30.118911	72.166478
647.387270	31.432130	72.171482
646.440731	25.625436	72.176487
645.747451	32.075059	72.181492
644.859980	26.837680	72.186497
644.866575	17.692293	72.191502
644.324515	30.636725	72.196506
643.338822	27.446033	72.201511
642.611865	29.435246	72.206516
641.980135	24.068836	72.211521
641.631442	24.058225	72.216526
640.183695	35.150543	72.221530
639.705083	30.936113	72.226535
639.614729	23.129179	72.231540
638.786999	37.218210	72.236545
638.225804	29.853673	72.241550
637.393201	31.602678	72.246554
636.738285	31.800102	72.251559
636.347907	29.596358	72.256564
635.067249	35.533999	72.261569
634.643496	32.100859	72.266574
634.017033	32.378905	72.271578
633.723806	28.533908	72.276583
632.845725	36.326522	72.281588
632.164943	33.812648	72.286593
631.786762	34.117384	72.291598
630.415886	30.037170	72.296602
629.909075	26.664567	72.301607
629.569421	27.808384	72.306612
628.909709	35.329687	72.311617
628.287529	27.925983	72.316622
627.159007	26.711821	72.321626
626.757205	29.526009	72.326631
626.393436	27.751677	72.331636
625.282684	36.639446	72.336641
624.715660	27.091839	72.341646
624.129891	36.083651	72.346650
623.765281	19.560733	72.351655
622.606668	31.931602	72.356660
621.654055	33.127311	72.361665
621.419645	29.008030	72.366670
620.802314	40.209374	72.371674
620.725121	35.915247	72.376679
619.746647	36.850157	72.381684
618.929993	40.506252	72.386689
618.316203	25.394915	72.391694
617.363278	28.342607	72.396698
616.589334	30.206851	72.401703
616.071639	39.705046	72.406708
615.390262	29.589047	72.411713
615.366205	23.720603	72.416718
614.223810	32.592914	72.421722
613.435994	30.837234	72.426727
613.134110	30.312989	72.431732
612.318873	30.651066	72.436737
611.550331	24.376085	72.441742
610.861273	34.563866	72.446746
610.435672	21.715374	72.451751
609.475767	27.925203	72.456756
608.750552	37.420180	72.461761
608.402171	32.134801	72.466766
607.813451	38.306018	72.471770
606.981871	30.158259	72.476775
606.011017	39.430595	72.481780
605.150398	39.536214	72.486785
605.278644	35.980472	72.491790
604.651443	30.186011	72.496794
603.693061	26.751298	72.501799
602.937298	28.317770	72.506804
602.325707	39.581277	72.511809
602.146850	35.197692	72.516814
600.876244	31.330176	72.521818
600.351309	22.294677	72.526823
599.886794	27.764889	72.531828
598.958506	28.109937	72.536833
597.988718	18.590225	72.541838
597.549742	37.168268	72.546842
597.288252	37.150082	72.551847
596.830717	24.663057	72.556852
595.598196	30.987271	72.561857
595.303692	18.110023	72.566862
594.499054	35.845895	72.571866
593.622757	28.992014	72.576871
592.773345	30.734248	72.581876
592.051744	23.791078	72.586881
592.139170	19.179014	72.591886
591.655792	28.611818	72.596890
590.609605	25.187942	72.601895
590.189992	36.657406	72.606900
588.731747	25.036219	72.611905
588.148216	25.941351	72.616910
587.386400	29.413683	72.621914
586.815278	27.555692	72.626919
586.602557	26.424336	72.631924
586.043354	32.404778	72.636929
585.630491	27.504977	72.641934
584.699037	22.932196	72.646938
584.128125	44.200947	72.651943
583.123950	26.529420	72.656948
581.945581	32.373524	72.661953
582.169423	25.732340	72.666958
581.615058	29.343513	72.671962
580.464076	30.698560	72.676967
579.664439	26.196245	72.681972
579.219877	34.832846	72.686977
578.748273	28.961572	72.691982
577.801593	32.736155	72.696986
576.774302	31.669889	72.701991
576.398082	31.706249	72.706996
575.980470	29.114206	72.712001
575.778868	24.724789	72.717006
574.779953	30.004166	72.722010
573.968247	32.743307	72.727015
573.742081	17.494566	72.732020
572.418512	32.640256	72.737025
571.735034	22.348001	72.742030
571.341751	34.697909	72.747034
570.760416	32.388979	72.752039
569.945551	36.252953	72.757044
569.184604	33.635176	72.762049
568.839004	35.390208	72.767054
568.300340	21.457487	72.772058
567.288195	18.512308	72.777063
566.394662	22.018239	72.782068
565.734910	44.862268	72.787073
565.650880	22.622572	72.792078
564.692577	31.821956	72.797082
563.476271	18.957507	72.802087
563.044770	23.909972	72.807092
562.384852	33.470246	72.812097
562.302858	29.107507	72.817102
561.718164	19.621087	72.822106
561.178083	20.208655	72.827111
560.538184	21.639993	72.832116
559.464012	31.400286	72.837121
558.555518	26.834895	72.842126
558.040468	25.266015	72.847130
557.633946	34.311281	72.852135
556.710871	34.598747	72.857140
555.653080	35.610968	72.862145
555.048772	28.768970	72.867150
554.832942	23.796794	72.872154
554.391763	18.800592	72.877159
553.621956	29.740806	72.882164
552.680439	29.660640	72.887169
552.037474	14.844138	72.892174
551.706394	27.948927	72.897178
551.085015	21.111230	72.902183
550.272832	18.627775	72.907188
549.777109	27.269370	72.912193
549.197839	28.137563	72.917198
548.028607	20.589226	72.922202
547.632731	19.714121	72.927207
547.103949	18.059125	72.932212
545.810387	18.951215	72.937217
545.198663	14.784823	72.942222
544.754447	27.997516	72.947226
544.322756	25.934406	72.952231
544.030864	20.368821	72.957236
542.824655	28.238953	72.962241
542.674394	21.324637	72.967246
541.643465	28.644896	72.972250
540.541693	32.382698	72.977255
540.508382	17.139514	72.982260
539.633673	29.372148	72.987265
538.945801	24.762161	72.992270
537.896205	29.595479	72.997274
537.077451	31.026930	73.002279
537.120969	34.959173	73.007284
536.093976	24.054624	73.012289
535.992214	23.785505	73.017294
534.934928	9.490738	73.022298
534.096181	25.219922	73.027303
533.857349	10.780587	73.032308
533.080227	26.818489	73.037313
532.369528	21.103585	73.042318
531.567485	24.382073	73.047322
531.397114	28.238003	73.052327
530.600067	23.954482	73.057332
529.530066	22.828812	73.062337
529.109963	20.536787	73.067342
528.491497	21.772337	73.072346
527.376219	31.346808	73.077351
526.870894	27.549807	73.082356
526.342838	24.920178	73.087361
526.257179	24.911836	73.092366
525.153354	28.254169	73.097370
524.222304	28.640684	73.102375
523.599146	20.997487	73.107380
523.242311	17.769748	73.112385
522.510194	28.565196	73.117390
521.284836	26.303682	73.122394
520.705136	20.618374	73.127399
520.492534	14.537134	73.132404
519.977512	23.008345	73.137409
519.474975	19.958353	73.142414
518.552141	23.976727	73.147418
518.102617	25.647398	73.152423
517.039460	19.233314	73.157428
516.206651	26.132527	73.162433
515.685887	13.750224	73.167438
515.327117	17.185173	73.172442
514.618689	29.123252	73.177447
513.704796	22.109823	73.182452
513.014415	36.293685	73.187457
512.727548	26.915944	73.192462
511.869965	36.887748	73.197466
510.924196	30.139582	73.202471
510.522074	26.572141	73.207476
510.019720	33.158529	73.212481
509.701145	20.076986	73.217486
508.417837	24.466591	73.222490
507.567006	26.713685	73.227495
507.401430	24.582958	73.232500
506.686177	21.048058	73.237505
506.005686	21.531854	73.242510
505.102839	31.145028	73.247514
504.558904	25.594369	73.252519
504.104885	23.057025	73.257524
502.865396	26.444633	73.262529
502.575700	21.386464	73.267534
502.358295	28.790017	73.272538
501.578050	21.493539	73.277543
500.487478	19.850783	73.282548
499.949695	27.188684	73.287553
499.597269	22.306083	73.292558
498.480532	14.741529	73.297562
497.648812	26.325525	73.302567
497.447853	28.538475	73.307572
497.038589	33.389642	73.312577
496.194074	27.409071	73.317582
495.344641	28.887998	73.322586
494.490285	34.138067	73.327591
494.432101	19.641569	73.332596
492.735451	34.457233	73.337601
492.687931	22.284955	73.342606
491.898602	21.445735	73.347610
491.564300	31.028257	73.352615
491.197712	18.066330	73.357620
489.925344	24.631891	73.362625
489.458721	36.337499	73.367630
488.767015	26.841339	73.372634
487.757520	29.419635	73.377639
487.660869	25.158583	73.382644
486.674335	23.762600	73.387649
486.241867	18.233613	73.392654
485.125827	18.406773	73.397658
484.054482	19.870597	73.402663
483.992616	23.280326	73.407668
483.502987	27.985029	73.412673
483.360026	19.973617	73.417678
482.102036	25.811521	73.422682
481.493453	23.489611	73.427687
481.191836	24.245778	73.432692
480.091538	25.271109	73.437697
479.318935	26.307309	73.442702
478.693051	19.418317	73.447706
478.288365	22.348096	73.452711
477.854713	16.190120	73.457716
476.589634	22.992637	73.462721
476.348393	23.453768	73.467726
475.871550	17.450901	73.472730
474.756814	20.708262	73.477735
474.482325	16.111284	73.482740
473.720516	10.697850	73.487745
472.937118	17.057785	73.492750
471.774167	25.648000	73.497754
470.980264	26.999821	73.502759
470.840435	21.654440	73.507764
470.114883	22.933872	73.512769
470.145301	22.041324	73.517774
468.629194	27.403136	73.522778
467.957199	28.861688	73.527783
467.989275	14.369742	73.532788
467.244378	21.576646	73.537793
466.172523	16.638370	73.542798
465.407448	22.405632	73.547802
465.123209	22.755348	73.552807
464.890383	30.208665	73.557812
463.684711	32.184314	73.562817
463.240626	29.588627	73.567822
462.150940	18.457576	73.572826
460.995208	31.033035	73.577831
460.501515	29.705192	73.582836
460.140825	19.025676	73.587841
459.997143	26.928396	73.592846
459.575224	25.257970	73.597850
458.384138	31.074189	73.602855
458.079047	26.087863	73.607860
457.166888	30.588665	73.612865
456.149872	28.910556	73.617870
455.633388	20.260096	73.622874
454.841610	29.622204	73.627879
454.728675	26.667841	73.632884
453.430171	32.710904	73.637889
453.116861	19.253238	73.642894
452.706141	28.978818	73.647898
451.734202	25.569983	73.652903
451.066247	17.339460	73.657908
450.218419	20.518037	73.662913
450.019743	23.074387	73.667918
449.258500	21.942134	73.672922
448.338561	26.005801	73.677927
447.727925	27.028819	73.682932
447.131012	31.898851	73.687937
446.261929	30.369057	73.692942
445.411451	25.291441	73.697946
444.910234	23.133777	73.702951
444.377102	18.835047	73.707956
443.976605	26.660418	73.712961
443.838486	23.694300	73.717966
442.847836	20.405142	73.722970
441.822673	23.848511	73.727975
441.562976	20.345122	73.732980
440.313661	28.416121	73.737985
439.755824	22.164402	73.742990
439.191401	28.358578	73.747994
438.325282	24.879275	73.752999
437.718745	25.920565	73.758004
437.012718	24.986091	73.763009
436.478939	24.178708	73.768014
436.073998	32.615048	73.773018
435.295495	30.660833	73.778023
434.527998	29.280432	73.783028
433.768021	31.290731	73.788033
433.284639	26.809039	73.793038
432.641397	28.076945	73.798042
431.515642	23.945180	73.803047
431.439525	16.962299	73.808052
430.921711	17.863303	73.813057
429.834573	21.748619	73.818062
428.944047	34.404832	73.823066
428.550894	29.941879	73.828071
428.401060	16.425059	73.833076
427.578122	22.751886	73.838081
426.674156	27.469002	73.843086
426.120420	17.555089	73.848090
425.478268	32.002498	73.853095
424.439268	28.287404	73.858100
424.016854	33.695741	73.863105
423.208219	18.391620	73.868110
422.926629	30.875113	73.873114
422.042653	29.983189	73.878119
421.470185	20.155836	73.883124
421.089977	35.518684	73.888129
420.312217	26.414718	73.893134
419.415826	29.582122	73.898138
418.731338	24.484376	73.903143
418.321044	16.482458	73.908148
417.072532	29.823315	73.913153
416.501429	29.042383	73.918158
416.108015	28.725128	73.923162
415.533100	31.264165	73.928167
415.020014	26.326758	73.933172
413.640470	30.138832	73.938177
413.188015	25.702678	73.943182
413.257184	26.417117	73.948186
411.685501	39.386872	73.953191
411.388747	31.783156	73.958196
410.625954	33.335035	73.963201
410.236046	31.426136	73.968206
410.219746	34.804953	73.973210
408.968708	28.690506	73.978215
408.498973	28.295531	73.983220
407.368644	26.480963	73.988225
406.345914	18.031032	73.993230
405.663600	22.055270	73.998234
404.985591	28.180822	74.003239
405.194105	28.317990	74.008244
404.601713	37.706688	74.013249
403.875855	26.453036	74.018254
402.843869	28.374229	74.023258
402.375014	27.911309	74.028263
401.761306	22.827520	74.033268
400.434078	31.308330	74.038273
400.190999	34.764283	74.043278
399.705324	31.479826	74.048282
398.620536	42.039778	74.053287
398.103149	33.868847	74.058292
397.383569	31.624568	74.063297
397.148309	26.936197	74.068302
396.647273	21.087009	74.073306
395.739408	32.030331	74.078311
394.948493	29.541964	74.083316
394.301343	32.086208	74.088321
393.711257	24.511897	74.093326
392.713567	23.838370	74.098330
392.103336	30.792033	74.103335
391.899371	18.099099	74.108340
390.937722	26.860686	74.113345
390.176850	34.298808	74.118350
389.867601	27.233234	74.123354
388.846061	25.803447	74.128359
388.601082	21.089820	74.133364
387.328138	31.239798	74.138369
387.247913	29.292593	74.143374
386.568128	29.632812	74.148378
385.493582	28.530006	74.153383
384.867220	19.345165	74.158388
384.375908	25.918768	74.163393
384.014082	20.974612	74.168398
383.144405	24.664452	74.173402
382.081144	26.202721	74.178407
381.771138	26.468246	74.183412
381.110842	30.561520	74.188417
380.552129	22.324650	74.193422
379.849567	26.449889	74.198426
379.174388	30.947643	74.203431
378.691988	21.586903	74.208436
377.438480	25.823594	74.213441
376.753038	29.886184	74.218446
376.174636	26.887737	74.223450
376.084382	30.295682	74.228455
375.687677	27.760270	74.233460
374.581082	31.032146	74.238465
373.834974	27.320862	74.243470
373.469763	18.931738	74.248474
372.006074	30.249059	74.253479
371.541172	20.268968	74.258484
370.810399	24.124325	74.263489
370.523304	25.415911	74.268494
370.548925	28.065828	74.273498
369.265630	34.464461	74.278503
368.722679	22.117276	74.283508
368.064721	21.536270	74.288513
366.929693	24.900986	74.293518
366.154828	29.127634	74.298522
365.517471	33.050106	74.303527
365.474948	20.774555	74.308532
364.882863	28.734540	74.313537
363.928228	29.626326	74.318542
363.501520	19.673266	74.323546
362.654305	32.615892	74.328551
361.655308	12.119476	74.333556
361.138085	24.847087	74.338561
360.648874	12.366774	74.343566
360.326436	11.850568	74.348570
359.094750	22.675194	74.353575
358.450149	17.929068	74.358580
357.950714	20.955960	74.363585
357.291083	13.143601	74.368590
356.422975	24.567851	74.373594
355.313379	26.474623	74.378599
355.299226	21.686370	74.383604
354.904540	17.416061	74.388609
354.465249	22.880705	74.393614
353.625124	17.782556	74.398618
352.545073	15.578396	74.403623
352.310286	2.910896	74.408628
351.487172	16.368466	74.413633
350.381620	23.289111	74.418638
349.790080	14.524497	74.423642
349.266100	26.480510	74.428647
349.018123	20.266165	74.433652
347.923516	11.865568	74.438657
347.327413	22.338180	74.443662
347.139693	22.065423	74.448666
345.961813	27.857506	74.453671
345.235158	19.533877	74.458676
344.449194	23.538380	74.463681
344.351322	18.829700	74.468686
343.822872	19.130043	74.473690
342.543899	27.986371	74.478695
342.173676	12.555658	74.483700
342.063123	18.447285	74.488705
340.776184	11.092863	74.493710
340.336543	11.005330	74.498714
339.512371	17.562600	74.503719
338.807411	25.649382	74.508724
338.138399	27.273064	74.513729
337.469339	22.820990	74.518734
337.174158	21.705954	74.523738
335.725847	25.095382	74.528743
335.320582	16.021975	74.533748
334.820931	26.890788	74.538753
334.618051	20.077924	74.543758
333.511109	23.163798	74.548762
332.446583	27.222162	74.553767
332.104454	24.646523	74.558772
331.453329	22.602660	74.563777
331.322895	30.326655	74.568782
330.356642	28.266786	74.573786
329.550052	23.045033	74.578791
329.027337	25.821762	74.583796
327.881120	25.723847	74.588801
327.439731	29.580401	74.593806
326.785179	25.379897	74.598810
325.970414	20.271409	74.603815
326.039318	28.703194	74.608820
324.699557	27.783028	74.613825
324.148982	14.962436	74.618830
323.512408	15.541780	74.623834
323.065246	19.553788	74.628839
322.725322	11.214266	74.633844
321.654912	29.240096	74.638849
321.224603	22.491865	74.643854
320.357241	9.761191	74.648858
319.379131	25.788579	74.653863
318.970897	17.598707	74.658868
318.200100	24.700968	74.663873
317.644802	27.691043	74.668878
317.090681	20.287638	74.673882
316.219100	26.295832	74.678887
315.891821	8.667985	74.683892
315.210201	20.956614	74.688897
314.073140	19.472736	74.693902
313.748995	15.563339	74.698906
313.136462	25.321090	74.703911
312.360200	18.605927	74.708916
311.404874	26.038787	74.713921
310.833778	18.556092	74.718926
310.709862	11.511463	74.723930
309.926190	28.349924	74.728935
309.066539	18.814378	74.733940
308.457705	16.847357	74.738945
307.642055	25.557314	74.743950
307.359638	19.968184	74.748954
306.134549	17.847084	74.753959
305.552143	18.923981	74.758964
305.042753	26.260537	74.763969
304.959991	19.620913	74.768974
303.984544	13.326995	74.773978
302.876782	16.813541	74.778983
302.870356	11.401191	74.783988
301.798030	27.650174	74.788993
300.743920	23.694706	74.793998
300.387976	22.490016	74.799002
299.948465	19.948828	74.804007
299.388145	10.978992	74.809012
298.408075	27.746260	74.814017
297.588255	34.255548	74.819022
297.461320	13.350525	74.824026
296.690012	26.336251	74.829031
295.672155	16.726585	74.834036
294.927827	28.219428	74.839041
294.476404	30.220008	74.844046
294.576379	28.455389	74.849050
293.450179	32.930439	74.854055
292.739783	27.477332	74.859060
291.818301	34.288244	74.864065
290.739965	30.249911	74.869070
290.239031	24.861186	74.874074
289.466300	21.613051	74.879079
289.342640	20.363454	74.884084
289.142709	17.801426	74.889089
288.212541	25.507816	74.894094
287.415742	24.297707	74.899098
286.521285	33.275691	74.904103
286.112734	31.872815	74.909108
285.236049	28.699594	74.914113
284.407268	34.145912	74.919118
284.065975	30.494707	74.924122
283.259190	30.919850	74.929127
282.156484	22.086928	74.934132
281.743182	32.823719	74.939137
281.195574	33.005709	74.944142
280.899651	28.284447	74.949146
279.972881	32.160033	74.954151
279.490594	18.262590	74.959156
278.500591	29.389336	74.964161
278.214081	23.945936	74.969166
277.978486	22.550185	74.974170
276.551702	26.287861	74.979175
276.259802	17.946998	74.984180
275.622180	26.614393	74.989185
274.378271	28.853259	74.994190
274.039300	19.263116	74.999194
273.028741	25.924232	75.004199
272.963722	20.724638	75.009204
272.312792	21.287361	75.014209
271.170772	16.806626	75.019214
270.879129	19.164924	75.024218
270.203362	25.394220	75.029223
269.384763	22.937118	75.034228
268.779537	25.621359	75.039233
268.057735	26.581718	75.044238
267.630056	24.727751	75.049242
266.519733	27.634427	75.054247
265.920157	25.468829	75.059252
265.816269	22.585576	75.064257
264.951624	24.745067	75.069262
264.356624	23.036039	75.074266
263.144082	28.340115	75.079271
262.706477	30.478841	75.084276
262.332312	20.138981	75.089281
261.531481	27.734880	75.094286
261.079144	26.372103	75.099290
260.076985	29.066006	75.104295
260.183816	29.175217	75.109300
258.645079	23.253371	75.114305
257.987505	30.299754	75.119310
257.821489	20.702544	75.124314
257.005689	27.651152	75.129319
256.565329	29.074410	75.134324
255.575673	20.255020	75.139329
254.728873	22.536243	75.144334
254.648177	22.656424	75.149338
253.312776	29.755669	75.154343
252.836806	21.198156	75.159348
252.629240	25.369093	75.164353
251.374985	30.082183	75.169358
250.892758	29.785421	75.174362
249.934905	38.027654	75.179367
249.777661	21.306228	75.184372
249.432461	33.550710	75.189377
248.218971	24.509970	75.194382
247.806175	34.638003	75.199386
246.888109	36.746095	75.204391
246.640148	22.194742	75.209396
245.823675	27.807834	75.214401
244.724455	31.386082	75.219406
244.620843	25.651768	75.224410
243.435620	23.043393	75.229415
242.585728	28.896770	75.234420
242.300974	29.522549	75.239425
241.636866	30.604601	75.244430
241.559586	28.019870	75.249434
240.259211	35.132462	75.254439
239.618590	25.238765	75.259444
239.361999	23.784866	75.264449
238.256828	25.394529	75.269454
237.648143	27.387074	75.274458
237.040157	25.866196	75.279463
236.525241	24.756241	75.284468
236.200452	29.491471	75.289473
235.049574	27.837951	75.294478
234.316225	28.128406	75.299482
234.077722	33.717171	75.304487
233.291116	23.707984	75.309492
232.306041	30.347706	75.314497
231.772959	27.277420	75.319502
231.535650	21.226968	75.324506
230.291516	31.813947	75.329511
229.632634	23.839088	75.334516
229.284455	18.539566	75.339521
228.650749	30.222936	75.344526
227.767316	18.179233	75.349530
226.994938	32.166471	75.354535
226.469948	20.557613	75.359540
225.995631	28.087276	75.364545
224.889390	22.880220	75.369550
224.524494	25.713807	75.374554
223.994448	29.158749	75.379559
223.349577	17.218938	75.384564
222.846410	22.980774	75.389569
222.141887	22.735225	75.394574
221.536419	15.048314	75.399578
220.521730	29.802703	75.404583
219.506788	25.278079	75.409588
218.766866	28.280260	75.414593
218.184735	17.227699	75.419598
218.240294	17.505924	75.424602
217.836571	28.783638	75.429607
216.559713	30.127380	75.434612
215.961373	30.121937	75.439617
215.300734	24.919536	75.444622
214.841858	21.410088	75.449626
213.656157	35.915793	75.454631
213.337002	30.969596	75.459636
212.916494	18.519375	75.464641
211.857519	31.620364	75.469646
211.615801	20.010504	75.474650
211.202812	23.225482	75.479655
209.840785	14.774555	75.484660
208.976786	30.034757	75.489665
208.569067	24.049322	75.494670
208.174284	20.595887	75.499674
207.301799	30.287871	75.504679
206.781429	19.175005	75.509684
206.124465	26.916708	75.514689
205.388660	32.401839	75.519694
204.993697	18.170392	75.524698
204.019987	30.040430	75.529703
203.275645	22.659502	75.534708
202.857429	28.915558	75.539713
202.195543	29.390163	75.544718
201.383521	22.527785	75.549722
200.510720	24.158761	75.554727
200.230317	22.017987	75.559732
199.477888	23.233974	75.564737
197.986827	34.669279	75.569742
197.659917	23.090348	75.574746
197.289803	27.796538	75.579751
197.310170	23.602008	75.584756
196.587109	28.291933	75.589761
195.210786	30.668637	75.594766
194.790892	29.671270	75.599770
194.358065	29.830249	75.604775
193.934874	26.457035	75.609780
192.711924	16.545821	75.614785
191.581777	25.856281	75.619790
191.508429	24.737434	75.624794
191.181356	35.558251	75.629799
190.207515	30.569788	75.634804
189.358504	28.231098	75.639809
188.943469	28.505508	75.644814
188.400998	23.946570	75.649818
187.025794	39.509054	75.654823
186.502201	21.109897	75.659828
186.135902	23.771831	75.664833
185.869799	35.659943	75.669838
184.886658	28.842196	75.674842
184.215736	27.165792	75.679847
183.532505	39.226063	75.684852
183.101928	32.343870	75.689857
182.109485	40.881787	75.694862
181.842182	21.410483	75.699866
181.220834	42.983726	75.704871
180.186745	38.429054	75.709876
179.596856	28.328600	75.714881
178.752863	23.407747	75.719886
178.465086	23.906287	75.724890
177.888134	27.404445	75.729895
176.924283	34.472871	75.734900
176.346758	21.642433	75.739905
175.995622	27.184503	75.744910
175.201209	28.304694	75.749914
174.269512	23.560247	75.754919
173.390265	25.397256	75.759924
173.180566	23.155330	75.764929
172.180257	35.119504	75.769934
171.408981	34.405238	75.774938
170.620534	26.528324	75.779943
170.225784	25.656258	75.784948
170.042402	27.797041	75.789953
169.154602	37.720130	75.794958
168.765918	26.434894	75.799962
168.047170	34.659525	75.804967
167.273592	31.324837	75.809972
166.758960	26.512317	75.814977
165.948738	27.087851	75.819982
164.734664	26.248655	75.824986
163.678696	39.062191	75.829991
163.347173	28.460095	75.834996
163.137604	23.587898	75.840001
162.700185	28.404167	75.845006
162.219071	29.371910	75.850010
161.341243	24.264079	75.855015
160.685028	31.212498	75.860020
159.967134	29.606666	75.865025
158.673387	25.435595	75.870030
158.406883	26.952569	75.875034
157.476610	28.833989	75.880039
157.333255	35.492486	75.885044
157.046227	37.384880	75.890049
155.589410	43.133218	75.895054
155.287059	33.835289	75.900058
154.724726	28.856918	75.905063
153.621110	39.017843	75.910068
152.635310	26.764997	75.915073
152.331453	25.903671	75.920078
152.280593	31.301677	75.925082
151.723274	32.264227	75.930087
150.681864	33.010665	75.935092
150.293383	33.791759	75.940097
149.170447	33.955132	75.945102
148.786997	35.724134	75.950106
147.764856	35.574981	75.955111
147.201411	29.872998	75.960116
146.866170	26.197200	75.965121
145.621371	38.996697	75.970126
145.159526	34.212031	75.975130
144.642817	43.738506	75.980135
144.067139	38.158314	75.985140
143.059964	39.966851	75.990145
142.182889	33.914347	75.995150
141.858692	29.500380	76.000154
141.123485	43.223105	76.005159
141.121313	37.529390	76.010164
140.300336	30.062935	76.015169
139.418784	35.736896	76.020174
139.238819	29.078095	76.025178
137.942074	40.818326	76.030183
136.979705	31.337076	76.035188
136.861814	28.938592	76.040193
136.159749	39.183721	76.045198
135.145417	33.495292	76.050202
134.285226	35.119551	76.055207
133.751368	32.599746	76.060212
133.616166	28.172991	76.065217
132.808209	26.854331	76.070222
131.956307	31.916463	76.075226
130.791475	35.587220	76.080231
130.904611	27.213334	76.085236
130.861700	25.493573	76.090241
129.709680	38.027556	76.095246
129.157575	30.007319	76.100250
128.272311	25.444713	76.105255
127.180566	38.842683	76.110260
126.679800	32.920983	76.115265
126.280446	33.082521	76.120270
125.513110	32.951090	76.125274
124.570875	29.963420	76.130279
123.972232	23.680456	76.135284
123.718847	26.313355	76.140289
122.743580	34.077449	76.145294
122.027295	21.746955	76.150298
121.196913	29.942088	76.155303
120.711405	27.966489	76.160308
120.719592	20.095025	76.165313
119.268532	34.931644	76.170318
118.920190	31.555971	76.175322
118.306819	40.255801	76.180327
117.654527	32.981642	76.185332
116.843128	27.199365	76.190337
115.545647	36.702115	76.195342
115.778729	39.470322	76.200346
115.360593	33.737291	76.205351
114.381673	38.527960	76.210356
113.544686	33.457786	76.215361
112.874276	40.157756	76.220366
112.354394	25.195653	76.225370
111.165453	27.570905	76.230375
110.706857	27.877505	76.235380
110.315773	26.640603	76.240385
110.187296	29.261468	76.245390
109.070825	34.890902	76.250394
108.249256	32.312910	76.255399
107.698719	34.340365	76.260404
107.256659	30.497111	76.265409
106.478603	45.548109	76.270414
105.567796	35.691233	76.275418
105.130942	38.712923	76.280423
103.845335	39.000026	76.285428
103.314801	29.175550	76.290433
102.809473	35.218439	76.295438
102.666800	37.245506	76.300442
102.023363	30.189130	76.305447
101.110660	29.394943	76.310452
100.197688	29.020251	76.315457
99.791332	42.368854	76.320462
99.020099	31.179331	76.325466
98.027290	32.627640	76.330471
97.436243	24.848583	76.335476
97.083464	18.457038	76.340481
96.736598	31.362500	76.345486
95.589330	33.461467	76.350490
94.761858	30.127515	76.355495
94.341858	27.321493	76.360500
94.083566	32.563350	76.365505
93.028182	28.149308	76.370510
92.101376	27.936091	76.375514
91.599979	30.545469	76.380519
91.014846	24.905307	76.385524
90.991727	32.527029	76.390529
89.843210	31.680570	76.395534
89.261585	26.880331	76.400538
88.687007	33.516136	76.405543
87.520457	30.543755	76.410548
86.834270	26.953896	76.415553
86.410175	30.391428	76.420558
85.958316	27.991017	76.425562
85.499198	31.680129	76.430567
84.617748	38.983018	76.435572
84.171668	32.749846	76.440577
83.231489	34.468876	76.445582
82.494283	33.288755	76.450586
82.000275	38.268597	76.455591
81.276417	34.069759	76.460596
80.987914	21.251609	76.465601
79.572557	30.558713	76.470606
79.343324	26.206881	76.475610
78.841876	28.966073	76.480615
77.675819	41.347780	76.485620
76.960008	26.221402	76.490625
76.521389	32.061275	76.495630
76.455371	30.988570	76.500634
75.018095	40.417445	76.505639
74.406235	34.852507	76.510644
74.136793	27.569346	76.515649
73.380112	30.180018	76.520654
72.490417	29.219753	76.525658
71.713035	23.906713	76.530663
70.883234	29.244447	76.535668
70.810467	27.348107	76.540673
70.311992	37.934499	76.545678
69.528524	23.438635	76.550682
68.833178	27.729948	76.555687
68.101695	19.229010	76.560692
67.185539	19.113449	76.565697
66.212881	29.698193	76.570702
65.908061	26.916383	76.575706
65.454059	19.274748	76.580711
64.915585	25.403346	76.585716
63.960158	27.099585	76.590721
63.120036	27.271507	76.595726
62.786986	29.201209	76.600730
62.452608	28.231227	76.605735
61.255229	25.654845	76.610740
61.014683	16.388091	76.615745
60.423180	34.116844	76.620750
59.574465	31.376050	76.625754
58.653862	31.948723	76.630759
58.041448	35.936668	76.635764
57.496637	28.380473	76.640769
56.228161	25.525286	76.645774
55.706013	25.395772	76.650778
55.255113	27.844144	76.655783
54.609454	35.561999	76.660788
54.701942	22.766666	76.665793
53.639475	34.479022	76.670798
53.108506	25.625998	76.675802
52.493182	24.238798	76.680807
51.328447	31.285688	76.685812
50.663078	29.598976	76.690817
50.041400	35.400243	76.695822
49.660504	30.053934	76.700826
48.984390	18.872926	76.705831
47.613493	31.334612	76.710836
47.487316	25.649647	76.715841
46.962484	29.640970	76.720846
46.560107	26.155662	76.725850
45.644257	29.488712	76.730855
44.960759	18.474456	76.735860
44.456309	29.665745	76.740865
43.074333	30.742501	76.745870
42.873847	29.595055	76.750874
42.309445	38.310739	76.755879
41.693987	40.887858	76.760884
40.866707	29.185352	76.765889
40.039611	33.174426	76.770894
39.550363	26.273245	76.775898
39.447081	28.888517	76.780903
38.111268	26.408341	76.785908
37.496326	28.233202	76.790913
36.682354	34.471978	76.795918
36.500421	26.104161	76.800922
35.743612	34.148817	76.805927
34.579432	28.301420	76.810932
34.558846	27.186780	76.815937
34.189753	31.038151	76.820942
33.253200	35.173990	76.825946
32.160283	30.665043	76.830951
31.537512	30.889038	76.835956
31.182057	19.000906	76.840961
29.977381	38.965726	76.845966
29.204368	18.822960	76.850970
29.078624	28.473150	76.855975
28.686884	33.510801	76.860980
28.347202	25.977089	76.865985
27.067646	29.287735	76.870990
26.413076	34.755222	76.875994
25.593524	32.364588	76.880999
24.404007	28.210084	76.886004
24.465445	19.458116	76.891009
23.615653	33.437236	76.896014
23.618119	28.091285	76.901018
22.728936	35.463228	76.906023
21.528424	35.730493	76.911028
21.417263	19.612032	76.916033
20.201755	30.341177	76.921038
19.761066	29.780803	76.926042
19.064707	32.323524	76.931047
18.585367	21.577898	76.936052
18.344357	22.958359	76.941057
17.134367	32.735764	76.946062
16.581012	31.018580	76.951066
16.002038	26.380359	76.956071
14.521885	41.620623	76.961076
14.140039	12.089769	76.966081
13.457702	26.578314	76.971086
13.050523	28.070433	76.976090
12.736308	22.525850	76.981095
11.988502	26.959580	76.986100
11.599330	22.045092	76.991105
10.598437	29.381240	76.996110
9.826807	31.872894	77.001114
9.124274	26.663051	77.006119
8.338823	28.010513	77.011124
8.135841	28.271628	77.016129
7.536332	19.202483	77.021134
6.487306	18.493154	77.026139
5.952470	21.931013	77.031143
5.344295	28.463384	77.036148
4.885294	27.489636	77.041153
3.737000	29.908914	77.046158