Mon Mar 08 18:25:33 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.869221	97.273179	0.000000
-0.692834	93.249258	0.005005
-0.881808	66.997452	0.010010
-2.367481	22.668559	0.015014
-6.493233	1.997785	0.020019
-12.181206	12.344297	0.025024
-16.789670	9.072574	0.030029
-21.512349	1.108940	0.035034
-25.662177	11.698967	0.040038
-29.379416	9.012050	0.045043
-33.223008	12.588164	0.050048
-36.411269	2.870723	0.055053
-40.428260	11.739708	0.060058
-43.933081	-1.640774	0.065062
-47.584196	7.956719	0.070067
-51.550080	11.093496	0.075072
-54.967280	7.764274	0.080077
-59.027260	1.639292	0.085082
-62.952670	11.471368	0.090086
-66.669421	18.245712	0.095091
-70.628085	13.774499	0.100096
-73.734964	-1.292029	0.105101
-78.339631	6.475491	0.110106
-81.510800	-0.470879	0.115110
-85.200396	-0.911911	0.120115
-89.361115	9.613725	0.125120
-92.953220	-2.022918	0.130125
-97.083814	9.852463	0.135130
-100.247110	-7.103582	0.140134
-104.387345	8.688734	0.145139
-108.315180	9.542518	0.150144
-111.740402	2.223579	0.155149
-115.643741	12.911613	0.160154
-119.047891	13.210375	0.165158
-122.854168	9.635836	0.170163
-126.940513	4.964329	0.175168
-130.390164	-3.843984	0.180173
-134.397307	9.207030	0.185178
-138.288837	5.482124	0.190182
-142.056274	-0.897537	0.195187
-145.752133	-6.418173	0.200192
-149.175228	-0.745503	0.205197
-153.331791	1.672844	0.210202
-157.273646	7.614375	0.215206
-161.045300	8.459092	0.220211
-165.146799	11.401659	0.225216
-168.350790	5.897180	0.230221
-172.633707	14.321551	0.235226
-175.838228	2.544348	0.240230
-179.337488	8.344328	0.245235
-183.101541	9.676699	0.250240
-186.511405	12.729696	0.255245
-190.768627	13.778096	0.260250
-194.624724	-0.616791	0.265254
-198.364357	1.164270	0.270259
-202.266282	8.742605	0.275264
-205.762750	8.939533	0.280269
-209.797658	16.092848	0.285274
-213.331760	7.429012	0.290278
-217.139175	8.544439	0.295283
-220.941317	17.772064	0.300288
-224.761904	7.316904	0.305293
-228.655704	9.915785	0.310298
-232.256681	4.088417	0.315302
-235.836723	4.686638	0.320307
-239.845209	7.538794	0.325312
-243.415606	4.868200	0.330317
-247.259240	11.959509	0.335322
-250.977245	6.554527	0.340326
-254.927652	5.441057	0.345331
-258.476825	16.580534	0.350336
-262.063371	-1.274347	0.355341
-266.304120	19.009443	0.360346
-269.706268	5.113057	0.365350
-273.307384	-1.218822	0.370355
-277.510732	-0.292405	0.375360
-281.147128	-1.843863	0.380365
-284.990041	5.852905	0.385370
-288.246860	13.836158	0.390374
-292.252637	1.570463	0.395379
-296.243911	4.267006	0.400384
-299.780903	4.790645	0.405389
-303.823854	8.971405	0.410394
-307.554734	-5.077430	0.415398
-311.330389	-7.462854	0.420403
-315.030004	8.606362	0.425408
-318.668524	3.302338	0.430413
-322.455221	5.893731	0.435418
-326.513580	-3.468362	0.440422
-330.212597	1.330861	0.445427
-333.875675	-1.627559	0.450432
-337.056275	1.726496	0.455437
-341.072765	0.645795	0.460442
-344.931815	4.880838	0.465446
-348.490936	-3.122806	0.470451
-352.685169	2.397296	0.475456
-356.495877	-2.418730	0.480461
-360.497032	8.466624	0.485466
-364.061142	13.572353	0.490470
-367.587852	-7.232765	0.495475
-371.389837	10.905962	0.500480
-375.281217	-4.277714	0.505485
-378.990006	1.535494	0.510490
-383.090020	-0.766492	0.515494
-386.702519	6.382735	0.520499
-389.939477	11.418922	0.525504
-393.764438	0.494846	0.530509
-397.915296	2.502711	0.535514
-401.800759	6.500799	0.540518
-405.425587	7.424951	0.545523
-409.180817	5.365987	0.550528
-412.694984	0.483781	0.555533
-416.322474	8.352922	0.560538
-420.245481	6.443761	0.565542
-423.849103	5.393463	0.570547
-428.073706	11.702251	0.575552
-431.747607	4.893409	0.580557
-435.442700	19.341054	0.585562
-439.013565	9.683703	0.590566
-442.576614	-3.098666	0.595571
-446.580844	9.157614	0.600576
-450.291738	0.475080	0.605581
-454.301711	0.998784	0.610586
-458.273512	12.385781	0.615590
-462.211901	6.365084	0.620595
-465.841161	8.024858	0.625600
-468.916125	10.401901	0.630605
-472.905023	8.009788	0.635610
-476.521255	3.845685	0.640614
-480.285971	0.966800	0.645619
-484.521291	7.980678	0.650624
-488.068684	2.752250	0.655629
-491.647741	7.734397	0.660634
-495.648130	6.703422	0.665638
-499.305508	4.704663	0.670643
-503.451036	16.040634	0.675648
-506.667704	8.244301	0.680653
-510.581314	7.294104	0.685658
-514.330011	3.674738	0.690662
-517.957566	3.765331	0.695667
-521.844583	10.734683	0.700672
-525.433244	6.020655	0.705677
-529.860895	12.030904	0.710682
-533.449820	8.058060	0.715686
-537.063895	9.332335	0.720691
-540.948116	14.167765	0.725696
-544.070641	4.536742	0.730701
-547.939169	10.367835	0.735706
-551.717605	4.567736	0.740710
-555.238587	4.937814	0.745715
-559.580547	9.811696	0.750720
-563.383231	9.491961	0.755725
-567.673883	14.053327	0.760730
-570.823732	4.034066	0.765734
-574.345892	4.543125	0.770739
-578.526667	15.519012	0.775744
-581.851053	6.358657	0.780749
-586.126728	14.833032	0.785754
-589.774404	16.726157	0.790758
-593.184060	7.663014	0.795763
-597.416359	16.985143	0.800768
-601.020333	16.696800	0.805773
-604.691586	13.408963	0.810778
-608.344432	12.942368	0.815782
-611.879378	11.178101	0.820787
-616.229799	8.575919	0.825792
-619.973259	5.391103	0.830797
-623.681998	4.747390	0.835802
-627.158213	12.384522	0.840806
-630.717847	-1.273249	0.845811
-634.846558	15.472060	0.850816
-638.054900	6.195484	0.855821
-642.237360	16.779106	0.860826
-646.114393	5.800706	0.865830
-649.481901	-1.310608	0.870835
-653.579812	3.891858	0.875840
-657.645825	9.822480	0.880845
-661.196365	15.438951	0.885850
-665.110567	6.691486	0.890854
-668.731210	7.695788	0.895859
-672.652126	10.693929	0.900864
-675.815578	9.351347	0.905869
-679.615796	16.661874	0.910874
-683.416512	10.242688	0.915878
-686.858347	17.109629	0.920883
-691.498365	5.346524	0.925888
-695.271745	2.010501	0.930893
-699.083936	0.259132	0.935898
-702.583374	10.792053	0.940902
-705.997798	15.986314	0.945907
-710.063932	7.547041	0.950912
-713.671437	-4.529225	0.955917
-717.678375	13.701082	0.960922
-721.364563	3.966430	0.965926
-725.018504	1.694677	0.970931
-728.790804	15.325632	0.975936
-732.122371	14.462553	0.980941
-736.041140	6.189003	0.985946
-740.123920	6.122460	0.990950
-744.037977	8.175077	0.995955
-747.815475	18.331477	1.000960
-751.362688	6.859030	1.005965
-755.022723	12.691819	1.010970
-758.699506	15.986958	1.015974
-762.566590	11.202685	1.020979
-766.297514	17.534074	1.025984
-770.159130	-1.285174	1.030989
-774.037158	4.942005	1.035994
-777.668769	8.971079	1.040998
-781.372640	4.274290	1.046003
-785.389212	3.730491	1.051008
-789.036800	9.275927	1.056013
-792.969775	9.338489	1.061018
-796.651823	7.640589	1.066022
-800.321362	3.014033	1.071027
-804.214198	11.116946	1.076032
-807.768712	4.570316	1.081037
-811.387001	10.622007	1.086042
-815.036616	3.297425	1.091046
-818.651108	0.251582	1.096051
-823.001265	15.316950	1.101056
-826.383477	-3.859501	1.106061
-830.752824	0.431067	1.111066
-834.205453	1.657909	1.116070
-837.519611	6.681790	1.121075
-842.030112	5.878016	1.126080
-845.221506	-4.039590	1.131085
-848.961004	3.122719	1.136090
-853.037192	4.695258	1.141094
-857.267217	7.834570	1.146099
-860.677227	4.125357	1.151104
-863.843068	-15.741581	1.156109
-867.647418	7.593977	1.161114
-871.693575	4.820638	1.166118
-875.290210	-6.965375	1.171123
-879.461186	-3.147953	1.176128
-882.898504	0.069668	1.181133
-886.832276	9.431284	1.186138
-890.607228	-3.411082	1.191142
-894.218759	-3.998948	1.196147
-898.095761	5.225881	1.201152
-901.580720	-3.943004	1.206157
-905.962004	-8.094493	1.211162
-909.621388	2.319205	1.216166
-912.886285	2.754522	1.221171
-916.640842	8.957457	1.226176
-920.245153	2.220283	1.231181
-924.308720	2.792771	1.236186
-928.267128	8.782326	1.241190
-932.084350	-0.287659	1.246195
-935.971770	9.426147	1.251200
-939.648174	16.479169	1.256205
-943.157491	6.965750	1.261210
-946.563976	7.540441	1.266214
-950.337775	-1.888095	1.271219
-954.606650	7.795274	1.276224
-958.442517	3.820007	1.281229
-962.214862	-4.832923	1.286234
-965.821576	-2.288224	1.291238
-969.483276	0.867635	1.296243
-973.227008	4.197457	1.301248
-976.699023	-0.706389	1.306253
-980.671131	-3.135005	1.311258
-984.518113	-1.244098	1.316262
-988.119988	-14.806202	1.321267
-992.331817	1.760566	1.326272
-996.281231	-3.847453	1.331277
-999.869687	-0.682761	1.336282
-1003.303103	-5.695233	1.341286
-1006.893442	-1.808028	1.346291
-1010.665569	1.166869	1.351296
-1014.733456	1.760704	1.356301
-1018.713061	7.646568	1.361306
-1022.234604	2.968319	1.366310
-1026.041625	-3.819836	1.371315
-1030.016608	-1.955691	1.376320
-1033.420168	-2.236001	1.381325
-1037.214638	2.921733	1.386330
-1040.679272	-0.729589	1.391334
-1044.695358	-1.643582	1.396339
-1048.803280	-4.468227	1.401344
-1052.221356	-7.551422	1.406349
-1055.891861	-1.837933	1.411354
-1059.914027	-3.755387	1.416358
-1063.242516	-14.270443	1.421363
-1067.073494	-1.127913	1.426368
-1070.975319	-11.950202	1.431373
-1075.322966	-10.609812	1.436378
-1079.063297	-1.551638	1.441382
-1082.511845	-7.121353	1.446387
-1086.114406	-1.967433	1.451392
-1089.676081	-7.476467	1.456397
-1093.730210	-4.353835	1.461402
-1097.553617	-2.483862	1.466406
-1101.139701	0.272195	1.471411
-1105.039076	-8.994065	1.476416
-1108.377350	-2.855853	1.481421
-1112.513364	-7.407281	1.486426
-1116.497219	2.331689	1.491430
-1120.298865	-4.588043	1.496435
-1123.668478	-0.243993	1.501440
-1127.240797	-3.819612	1.506445
-1131.277054	-13.756166	1.511450
-1135.048218	3.185013	1.516454
-1138.848719	-7.044699	1.521459
-1142.838099	-2.260872	1.526464
-1146.285455	-0.876731	1.531469
-1149.747928	-10.510833	1.536474
-1153.752903	-4.686921	1.541478
-1157.636157	-10.328890	1.546483
-1161.605475	7.550727	1.551488
-1164.912024	1.978916	1.556493
-1168.692407	-2.067945	1.561498
-1172.152146	-3.949037	1.566502
-1176.252639	-10.447142	1.571507
-1180.383652	-4.558869	1.576512
-1184.262191	-8.785528	1.581517
-1188.122813	-11.999550	1.586522
-1191.272838	-0.665638	1.591526
-1194.765784	-10.876652	1.596531
-1199.145637	0.805423	1.601536
-1202.579105	-14.054210	1.606541
-1206.516486	-1.044248	1.611546
-1210.378851	-7.865805	1.616550
-1214.183557	-7.012554	1.621555
-1217.995056	-4.201330	1.626560
-1221.398726	-2.615925	1.631565
-1225.463495	-2.408552	1.636570
-1229.046645	-4.593066	1.641574
-1232.682542	-3.301624	1.646579
-1236.690393	-4.878881	1.651584
-1240.112448	-5.055009	1.656589
-1244.272450	-11.600233	1.661594
-1247.676492	-7.141698	1.666598
-1251.451295	-2.448794	1.671603
-1255.652563	-9.107236	1.676608
-1258.946711	-16.294007	1.681613
-1262.679832	-9.806989	1.686618
-1266.887633	-1.126280	1.691622
-1270.521290	-8.840566	1.696627
-1274.460702	4.430013	1.701632
-1277.967141	-7.305108	1.706637
-1281.828096	-1.945551	1.711642
-1285.176611	-15.640729	1.716646
-1289.022412	-1.301815	1.721651
-1293.123418	-6.024085	1.726656
-1296.904552	-12.729187	1.731661
-1300.715374	5.063773	1.736666
-1304.358375	-3.998754	1.741670
-1307.719631	-7.183693	1.746675
-1311.958247	0.685216	1.751680
-1315.254862	-8.995667	1.756685
-1319.343998	-7.295678	1.761690
-1323.492669	9.482287	1.766694
-1327.059977	0.961157	1.771699
-1330.969878	-5.887273	1.776704
-1333.834601	-11.912721	1.781709
-1337.722117	3.532016	1.786714
-1341.927212	2.257732	1.791718
-1345.421549	-5.469270	1.796723
-1349.537655	-5.124160	1.801728
-1353.145112	-2.687556	1.806733
-1357.016454	-9.616222	1.811738
-1360.458112	-4.197507	1.816742
-1364.321585	-6.909334	1.821747
-1368.438906	-1.338299	1.826752
-1371.784531	-12.200196	1.831757
-1376.200575	-6.647558	1.836762
-1379.622091	-1.790246	1.841766
-1383.199791	-10.317497	1.846771
-1387.085379	-3.943064	1.851776
-1390.505600	-11.519440	1.856781
-1394.616298	-2.513455	1.861786
-1398.175011	-2.719508	1.866790
-1401.846125	-10.958979	1.871795
-1405.948421	4.100802	1.876800
-1409.747137	-8.358391	1.881805
-1413.541895	-2.354824	1.886810
-1417.111761	-10.329798	1.891814
-1420.845118	-9.601165	1.896819
-1424.608421	5.106349	1.901824
-1428.015072	-8.093629	1.906829
-1432.454972	-4.615359	1.911834
-1436.214197	-1.618198	1.916838
-1439.605737	-12.947269	1.921843
-1443.340903	1.266940	1.926848
-1447.074191	-1.758885	1.931853
-1450.881539	-0.423883	1.936858
-1454.966250	0.176569	1.941862
-1458.253946	2.210500	1.946867
-1462.529229	9.147319	1.951872
-1465.973317	-2.770932	1.956877
-1469.855714	2.726396	1.961882
-1473.678577	5.582430	1.966886
-1477.029028	-8.183096	1.971891
-1481.310836	1.137422	1.976896
-1484.686270	-9.648567	1.981901
-1488.543433	-8.724969	1.986906
-1492.729478	1.709261	1.991910
-1495.936147	-11.934184	1.996915
-1500.166996	-7.012342	2.006912
-1501.121528	3.106454	2.016909
-1498.171929	-4.140708	2.026906
-1495.540445	-5.517204	2.036902
-1493.486664	-0.149403	2.046899
-1491.682366	-5.495346	2.056896
-1489.871524	-4.923146	2.066893
-1487.988468	-3.164143	2.076890
-1486.150882	-4.151411	2.086886
-1484.076371	-6.869165	2.096883
-1482.161701	-6.706723	2.106880
-1480.345837	-5.025372	2.116877
-1478.079994	-5.882270	2.126874
-1476.454166	-7.789261	2.136870
-1474.592786	-11.759659	2.146867
-1472.844556	-7.070775	2.156864
-1470.754394	-5.213874	2.166861
-1468.745918	-2.265522	2.176858
-1467.025356	-4.133994	2.186854
-1465.270380	-9.503597	2.196851
-1462.956679	-8.323504	2.206848
-1461.527264	-7.628632	2.216845
-1459.532589	-2.983932	2.226842
-1457.662948	-5.714648	2.236838
-1455.439176	-5.386949	2.246835
-1453.635643	0.993545	2.256832
-1452.061929	-2.888150	2.266829
-1450.023452	-1.180841	2.276826
-1448.145298	-5.652831	2.286822
-1446.183457	-6.836795	2.296819
-1444.568945	-7.976199	2.306816
-1442.603004	-4.346835	2.316813
-1440.396147	-4.715853	2.326810
-1438.719060	-5.746857	2.336806
-1436.744723	-4.973433	2.346803
-1434.966479	2.461076	2.356800
-1432.982890	7.540191	2.366797
-1431.299182	-0.937836	2.376794
-1429.272280	0.596090	2.386790
-1427.445541	-4.505517	2.396787
-1425.464411	-4.025262	2.406784
-1423.633817	-5.158196	2.416781
-1421.849579	-0.438719	2.426778
-1420.059707	1.859445	2.436774
-1418.012087	2.674835	2.446771
-1416.199720	5.015190	2.456768
-1414.371501	2.826376	2.466765
-1412.177212	0.384756	2.476762
-1410.638729	4.488356	2.486758
-1408.440927	4.119239	2.496755
-1406.665664	10.613245	2.506752
-1404.850304	2.592556	2.516749
-1402.900506	2.463664	2.526746
-1401.227955	1.785502	2.536742
-1399.385104	2.081084	2.546739
-1397.519394	-0.604748	2.556736
-1395.441192	10.372139	2.566733
-1393.728485	2.503674	2.576730
-1391.650817	5.875212	2.586726
-1389.612098	0.223405	2.596723
-1387.997693	2.802304	2.606720
-1386.271764	0.591995	2.616717
-1384.037658	0.594440	2.626714
-1382.200921	3.246695	2.636710
-1380.450265	3.822302	2.646707
-1378.542300	10.509816	2.656704
-1376.600044	5.415013	2.666701
-1375.033203	3.708577	2.676698
-1372.967876	4.368022	2.686694
-1371.048002	5.347581	2.696691
-1369.176900	7.302799	2.706688
-1367.435538	6.430497	2.716685
-1365.189955	2.938652	2.726682
-1363.654451	6.365425	2.736678
-1361.732259	2.836933	2.746675
-1359.786047	-0.553303	2.756672
-1358.282804	9.287292	2.766669
-1355.832494	2.349156	2.776666
-1354.045841	3.683197	2.786662
-1352.232958	7.883436	2.796659
-1350.464301	2.506983	2.806656
-1348.364157	3.337711	2.816653
-1346.688810	0.761333	2.826650
-1344.801511	3.062910	2.836646
-1342.962783	3.584976	2.846643
-1341.079973	7.909815	2.856640
-1339.061373	6.026886	2.866637
-1337.188727	7.595060	2.876634
-1335.153442	6.074184	2.886630
-1333.586629	2.773115	2.896627
-1331.465017	-2.940857	2.906624
-1329.720405	5.449609	2.916621
-1328.086152	8.341152	2.926618
-1326.153493	3.175298	2.936614
-1323.933579	1.997495	2.946611
-1322.128852	-0.238012	2.956608
-1320.479999	7.450981	2.966605
-1318.412432	1.232534	2.976602
-1316.500837	-0.990074	2.986598
-1314.899562	-0.182096	2.996595
-1313.068068	5.892479	3.006592
-1310.898344	2.032317	3.016589
-1308.756387	-3.501742	3.026586
-1307.202034	2.849288	3.036582
-1305.361941	8.235684	3.046579
-1303.651266	6.550482	3.056576
-1301.732366	5.772966	3.066573
-1299.769161	8.487151	3.076570
-1297.846399	8.034269	3.086566
-1295.815985	7.573633	3.096563
-1293.887040	-2.154553	3.106560
-1292.113208	4.142416	3.116557
-1290.309480	7.774197	3.126554
-1288.767881	4.595608	3.136550
-1286.495406	1.464253	3.146547
-1284.586264	0.055184	3.156544
-1282.902912	2.477870	3.166541
-1280.909434	4.805138	3.176538
-1279.171204	2.043487	3.186534
-1277.332550	5.374439	3.196531
-1275.301713	6.000020	3.206528
-1273.497356	6.616060	3.216525
-1271.434245	8.336957	3.226522
-1269.726274	6.592215	3.236518
-1267.724309	8.551838	3.246515
-1265.949219	11.079852	3.256512
-1264.034478	7.751566	3.266509
-1262.090325	12.245071	3.276506
-1260.263081	5.253586	3.286502
-1258.579109	3.586901	3.296499
-1256.259107	7.186615	3.306496
-1254.806508	8.034216	3.316493
-1252.833465	4.275051	3.326490
-1250.933839	2.243875	3.336486
-1249.098032	-0.430741	3.346483
-1247.097612	0.723919	3.356480
-1245.242962	1.235621	3.366477
-1243.428809	5.933093	3.376474
-1241.579780	0.436492	3.386470
-1239.502840	1.487339	3.396467
-1237.775081	4.513979	3.406464
-1235.996614	7.445668	3.416461
-1233.881955	7.492634	3.426458
-1232.159154	-0.112088	3.436454
-1230.445125	0.739482	3.446451
-1228.505848	1.243972	3.456448
-1226.517266	-3.512350	3.466445
-1224.468694	-1.710141	3.476442
-1222.852298	2.343231	3.486438
-1220.680432	-4.805992	3.496435
-1219.133818	-4.530756	3.506432
-1217.296657	7.283791	3.516429
-1215.088002	2.988031	3.526426
-1213.182193	4.640996	3.536422
-1211.520022	-1.990894	3.546419
-1209.649257	1.698116	3.556416
-1207.761079	2.183959	3.566413
-1205.968031	12.900366	3.576410
-1204.377370	2.730601	3.586406
-1201.910797	6.205872	3.596403
-1200.189117	3.405875	3.606400
-1198.370826	1.615113	3.616397
-1196.274841	1.699837	3.626394
-1194.598629	2.145398	3.636390
-1192.762955	7.022619	3.646387
-1190.936018	-0.396641	3.656384
-1188.953182	3.246037	3.666381
-1187.020811	5.453697	3.676378
-1185.291190	-1.758944	3.686374
-1183.434360	2.939643	3.696371
-1181.116400	0.802120	3.706368
-1179.703159	1.717641	3.716365
-1177.885445	2.473718	3.726362
-1175.755594	1.706763	3.736358
-1173.897366	4.504166	3.746355
-1172.151019	0.239781	3.756352
-1170.337995	0.960300	3.766349
-1168.356501	8.353048	3.776346
-1166.311256	4.468722	3.786342
-1164.599570	6.594871	3.796339
-1162.949188	0.533293	3.806336
-1160.812892	7.444986	3.816333
-1158.787544	10.749327	3.826330
-1157.000307	5.763177	3.836326
-1155.260115	2.657106	3.846323
-1153.660125	2.477024	3.856320
-1151.383153	4.806418	3.866317
-1149.550466	7.868443	3.876314
-1147.832972	5.198621	3.886310
-1145.605878	1.635731	3.896307
-1143.808609	1.228315	3.906304
-1142.035254	4.197210	3.916301
-1140.302108	7.210433	3.926298
-1138.430161	2.206008	3.936294
-1136.478107	3.804273	3.946291
-1134.305538	3.963640	3.956288
-1132.896907	7.796118	3.966285
-1130.764003	4.789865	3.976282
-1128.766084	2.874109	3.986278
-1127.350804	7.693905	3.996275
-1124.982470	1.489079	4.006272
-1123.355496	4.882441	4.016269
-1121.409208	5.824828	4.026266
-1119.481675	5.985514	4.036262
-1117.549166	7.181150	4.046259
-1115.792584	8.103364	4.056256
-1114.048604	6.221927	4.066253
-1112.195438	16.865648	4.076250
-1110.100382	7.152067	4.086246
-1108.063489	-0.910168	4.096243
-1106.307776	7.625549	4.106240
-1104.411197	8.727475	4.116237
-1102.863411	5.761161	4.126234
-1100.973411	4.723180	4.136230
-1098.954086	6.441764	4.146227
-1097.105296	0.901099	4.156224
-1094.966993	5.265802	4.166221
-1093.348450	1.306114	4.176218
-1091.213012	2.797719	4.186214
-1089.535810	2.668485	4.196211
-1087.486000	6.014764	4.206208
-1085.793165	0.559051	4.216205
-1083.866566	-0.688446	4.226202
-1081.925020	3.497751	4.236198
-1080.153156	0.309303	4.246195
-1078.503972	3.849139	4.256192
-1076.286791	3.772486	4.266189
-1074.373063	-0.913323	4.276186
-1072.662032	-4.414126	4.286182
-1070.933159	-4.436352	4.296179
-1068.817784	-0.004803	4.306176
-1066.856952	-0.302538	4.316173
-1065.306013	4.847690	4.326170
-1063.291589	3.895624	4.336166
-1061.140860	0.065564	4.346163
-1059.310385	-1.262849	4.356160
-1058.005495	-1.111468	4.366157
-1055.673242	-3.083795	4.376154
-1053.860964	-2.322014	4.386150
-1052.063249	-1.403173	4.396147
-1050.384304	-0.938998	4.406144
-1048.230820	2.367051	4.416141
-1046.282139	-2.198016	4.426138
-1044.376545	1.258206	4.436134
-1042.503649	-4.226276	4.446131
-1040.514205	-5.793249	4.456128
-1038.874288	0.387985	4.466125
-1037.030942	-0.437228	4.476122
-1035.297201	3.884872	4.486118
-1033.022834	-4.853150	4.496115
-1031.145190	3.456295	4.506112
-1029.491024	-4.449934	4.516109
-1027.520750	0.172223	4.526106
-1026.054131	-5.198326	4.536102
-1023.905411	-2.576726	4.546099
-1021.854926	3.818323	4.556096
-1020.206148	-1.835555	4.566093
-1018.364016	-1.624814	4.576090
-1016.123218	1.937291	4.586086
-1014.377381	3.008136	4.596083
-1012.589507	5.062219	4.606080
-1010.792880	3.650838	4.616077
-1008.797855	9.026920	4.626074
-1007.304226	3.311021	4.636070
-1004.887929	3.499423	4.646067
-1003.128124	6.817950	4.656064
-1001.374436	9.684318	4.666061
-999.662354	7.321768	4.676058
-997.550430	9.054054	4.686054
-995.827676	2.797857	4.696051
-993.748421	-1.983831	4.706048
-991.972303	1.251572	4.716045
-989.993069	10.271097	4.726042
-988.371378	2.377977	4.736038
-986.412952	-0.904971	4.746035
-984.446097	6.266088	4.756032
-982.483226	-2.437868	4.766029
-980.641274	2.545890	4.776026
-978.827338	4.880030	4.786022
-976.813982	2.774045	4.796019
-975.390997	7.073258	4.806016
-973.054451	4.587188	4.816013
-971.294016	6.410438	4.826010
-969.542760	1.436491	4.836006
-967.390951	-1.591587	4.846003
-965.786629	1.410792	4.856000
-963.721563	1.799078	4.865997
-961.835523	3.845398	4.875994
-960.068290	2.928209	4.885990
-958.037964	-3.692917	4.895987
-956.564131	5.637967	4.905984
-954.296680	5.877062	4.915981
-952.507961	6.731107	4.925978
-950.538761	-3.486406	4.935974
-949.005893	-2.934067	4.945971
-946.974812	0.554275	4.955968
-944.917356	1.959015	4.965965
-943.114736	1.476689	4.975962
-941.438015	5.083274	4.985958
-939.184870	3.006872	4.995955
-937.418415	2.528754	5.005952
-935.759372	6.187115	5.015949
-933.921123	4.398100	5.025946
-932.125988	0.850789	5.035942
-929.912902	4.802658	5.045939
-928.168913	-4.152038	5.055936
-926.149915	1.068710	5.065933
-924.430257	-5.117470	5.075930
-922.523241	-2.225033	5.085926
-920.464595	-8.118054	5.095923
-918.885664	-1.129643	5.105920
-916.894404	2.404566	5.115917
-915.032981	1.317621	5.125914
-912.859378	-2.804901	5.135910
-911.136126	-0.734092	5.145907
-909.734751	-6.504652	5.155904
-907.523358	-6.714425	5.165901
-905.546708	-6.403528	5.175898
-903.568830	1.858426	5.185894
-901.974150	-2.485727	5.195891
-899.936406	-3.057715	5.205888
-898.247899	-1.786571	5.215885
-896.491966	1.122148	5.225882
-894.364317	2.411505	5.235878
-892.437879	0.984196	5.245875
-890.587412	-7.371732	5.255872
-888.677206	-6.093396	5.265869
-886.904246	-0.702231	5.275866
-884.717773	-4.054712	5.285862
-883.359000	2.668937	5.295859
-881.386777	-6.830616	5.305856
-879.143376	-3.502466	5.315853
-877.504374	-12.266664	5.325850
-875.458445	-5.104995	5.335846
-873.793556	3.145448	5.345843
-871.901437	-4.413476	5.355840
-870.094109	0.544331	5.365837
-867.997399	-1.893822	5.375834
-866.423490	-3.391064	5.385830
-864.469739	-8.923074	5.395827
-862.493889	-13.703907	5.405824
-860.465923	-14.365873	5.415821
-858.717134	-8.383480	5.425818
-856.917954	-9.108339	5.435814
-854.941607	-5.914310	5.445811
-852.901631	-6.273465	5.455808
-851.215241	-6.943975	5.465805
-849.359040	-2.312898	5.475802
-847.538183	-0.265538	5.485798
-845.900098	-3.355066	5.495795
-843.815556	-8.731133	5.505792
-841.854000	2.528630	5.515789
-839.679426	-3.594429	5.525786
-838.303050	-0.820775	5.535782
-836.345126	-4.689288	5.545779
-834.030732	-6.339609	5.555776
-832.386265	-1.734671	5.565773
-830.683458	0.004744	5.575770
-828.719372	-2.028507	5.585766
-826.687636	-7.579269	5.595763
-825.028447	0.514234	5.605760
-822.950941	1.434318	5.615757
-821.182867	-0.247082	5.625754
-819.427589	1.616580	5.635750
-817.625499	-0.226564	5.645747
-815.403437	-4.378851	5.655744
-813.773991	-5.963879	5.665741
-811.719368	-0.631884	5.675738
-809.886881	4.164065	5.685734
-807.953649	-6.824405	5.695731
-806.408383	-6.545522	5.705728
-804.484599	-1.917315	5.715725
-802.495344	-7.260750	5.725722
-800.439339	-0.080092	5.735718
-798.485421	-6.763086	5.745715
-796.712487	-3.073881	5.755712
-795.027782	-3.720399	5.765709
-793.318014	-8.098666	5.775706
-791.436632	3.655519	5.785702
-789.169255	3.626376	5.795699
-787.181180	-0.788476	5.805696
-785.526328	-2.440702	5.815693
-783.869974	-1.446956	5.825690
-782.020019	0.709485	5.835686
-779.774022	2.782106	5.845683
-777.769489	2.981291	5.855680
-775.833192	5.196567	5.865677
-774.427720	-2.066625	5.875674
-772.454496	-5.623335	5.885670
-770.812689	-0.659518	5.895667
-768.586096	-5.545088	5.905664
-766.840007	-2.091560	5.915661
-764.937485	1.449071	5.925658
-762.844112	-3.067850	5.935654
-760.845574	1.731600	5.945651
-759.226764	-4.670450	5.955648
-757.574656	2.055346	5.965645
-755.819490	1.762318	5.975642
-753.711629	-0.034912	5.985638
-751.856750	5.108019	5.995635
-749.642822	-4.526378	6.005632
-747.947627	-3.006730	6.015629
-746.162562	-0.734104	6.025626
-744.319757	3.313437	6.035622
-742.570457	-1.257425	6.045619
-740.575636	-2.562913	6.055616
-738.652302	-0.623418	6.065613
-736.752551	-2.019496	6.075610
-734.702334	0.886529	6.085606
-733.166584	2.272202	6.095603
-731.136673	5.473570	6.105600
-729.339404	1.839225	6.115597
-727.349535	1.017678	6.125594
-725.435310	-0.050717	6.135590
-723.743338	5.620357	6.145587
-721.726305	-0.774258	6.155584
-719.872045	3.571461	6.165581
-717.980292	8.605902	6.175578
-716.042169	0.883426	6.185574
-714.344558	-0.576645	6.195571
-712.274249	-4.335130	6.205568
-710.527061	-11.150804	6.215565
-708.661234	-6.967973	6.225562
-706.811562	-2.716245	6.235558
-704.961540	-5.067471	6.245555
-702.793283	-0.505082	6.255552
-701.216993	-1.273152	6.265549
-699.167659	1.397792	6.275546
-697.264712	3.389525	6.285542
-695.289502	-0.135864	6.295539
-693.736446	-4.684807	6.305536
-691.568844	-9.845081	6.315533
-689.587556	-2.881319	6.325530
-688.361847	10.558202	6.335526
-686.272128	-2.405118	6.345523
-684.069090	1.300713	6.355520
-682.288852	-3.646088	6.365517
-680.223127	-0.890908	6.375514
-678.792567	-1.766725	6.385510
-676.859457	-7.104249	6.395507
-674.759986	-5.207055	6.405504
-672.927059	-2.962546	6.415501
-671.090134	-3.066477	6.425498
-669.358519	-0.104751	6.435494
-667.146773	-3.034778	6.445491
-665.302416	-13.048981	6.455488
-663.596667	-3.799153	6.465485
-661.968257	-5.748637	6.475482
-659.651391	1.021017	6.485478
-658.008781	-8.913584	6.495475
-656.258913	-7.655226	6.505472
-654.014483	-7.167436	6.515469
-652.284811	-4.579583	6.525466
-650.546758	-2.422525	6.535462
-648.801057	-6.924853	6.545459
-646.642098	-8.839097	6.555456
-644.711290	-11.171606	6.565453
-642.897711	-9.535012	6.575450
-641.063967	-5.384892	6.585446
-639.157231	-6.590963	6.595443
-637.352812	-5.634979	6.605440
-635.580012	-1.991413	6.615437
-633.588584	-4.174132	6.625434
-631.753438	-8.060762	6.635430
-629.670827	-2.733070	6.645427
-627.902594	-14.028195	6.655424
-625.979676	-8.870771	6.665421
-624.064463	-10.345016	6.675418
-622.532685	-7.030816	6.685414
-620.417623	-9.045387	6.695411
-618.737381	-5.500702	6.705408
-616.354774	-6.607522	6.715405
-614.768706	-4.661411	6.725402
-612.867059	-6.124007	6.735398
-611.080571	-5.575649	6.745395
-609.420896	-3.715501	6.755392
-607.150833	-5.333260	6.765389
-605.320052	-0.806861	6.775386
-603.735239	-11.433222	6.785382
-601.717654	-5.997226	6.795379
-599.734595	-6.932838	6.805376
-597.580323	-5.379053	6.815373
-596.284655	-4.813852	6.825370
-594.441547	-5.267647	6.835366
-592.312034	-7.669751	6.845363
-590.119991	-6.865649	6.855360
-588.386184	-4.330512	6.865357
-586.690198	-14.208860	6.875354
-584.697942	-9.146157	6.885350
-583.191382	-2.393820	6.895347
-581.177405	-6.905800	6.905344
-578.785801	-10.791284	6.915341
-577.371217	-11.433971	6.925338
-575.575491	-2.098972	6.935334
-573.552896	-6.024977	6.945331
-571.505046	-12.675436	6.955328
-569.536261	-4.735394	6.965325
-567.736119	-6.819611	6.975322
-566.157521	-8.549504	6.985318
-564.381718	-5.506339	6.995315
-562.313205	-10.194377	7.005312
-560.368590	-9.481772	7.015309
-558.329397	-8.814272	7.025306
-556.875625	-8.512716	7.035302
-554.835868	-12.289872	7.045299
-553.090164	-2.572668	7.055296
-550.802022	-4.359046	7.065293
-549.120012	-6.995938	7.075290
-547.457253	-6.138832	7.085286
-545.592039	-1.071589	7.095283
-543.379722	-1.612736	7.105280
-541.564920	-9.436957	7.115277
-539.645618	0.727778	7.125274
-537.679810	-5.663247	7.135270
-536.167144	-9.768289	7.145267
-533.976836	-13.443163	7.155264
-532.167615	-7.711729	7.165261
-530.597718	-9.059696	7.175258
-528.650404	-1.910367	7.185254
-526.787271	4.278238	7.195251
-524.615237	-9.419657	7.205248
-522.839511	-10.281039	7.215245
-520.808859	-5.562293	7.225242
-519.287484	-16.438989	7.235238
-517.355404	-7.984637	7.245235
-515.260970	-4.267614	7.255232
-513.210935	-5.469632	7.265229
-511.762507	-9.761761	7.275226
-509.836872	1.281431	7.285222
-507.930752	-3.366418	7.295219
-505.423487	-2.866782	7.305216
-504.303051	-3.552445	7.315213
-502.482057	3.347095	7.325210
-500.330140	-6.188775	7.335206
-498.558102	0.271760	7.345203
-496.236586	-5.293443	7.355200
-494.723354	-2.165659	7.365197
-493.168456	0.312863	7.375194
-490.887487	-0.002366	7.385190
-489.149067	2.483165	7.395187
-487.091491	0.286843	7.405184
-485.193570	-11.022593	7.415181
-483.601727	-11.682481	7.425178
-481.664388	-0.581136	7.435174
-479.341954	1.500095	7.445171
-477.727490	-2.704853	7.455168
-476.279134	2.291657	7.465165
-474.077652	-3.289092	7.475162
-472.289392	-0.033115	7.485158
-470.337048	-4.058341	7.495155
-468.422105	-1.588354	7.505152
-466.547485	-6.572181	7.515149
-464.605761	1.951735	7.525146
-463.135058	6.387339	7.535142
-460.760152	-0.705252	7.545139
-458.839367	0.480172	7.555136
-456.991943	1.388377	7.565133
-455.091209	-0.036057	7.575130
-453.457127	-1.651584	7.585126
-451.792323	6.566053	7.595123
-449.847284	-0.618932	7.605120
-447.882646	5.424063	7.615117
-445.606385	8.561085	7.625114
-444.144149	5.329378	7.635110
-441.958037	0.594237	7.645107
-440.387393	1.012987	7.655104
-438.469377	-0.494718	7.665101
-436.569262	-3.016368	7.675098
-434.762940	-1.830013	7.685094
-432.841078	3.214071	7.695091
-430.812421	2.092901	7.705088
-428.755428	-2.703713	7.715085
-427.291022	-1.581173	7.725082
-425.361093	-3.689169	7.735078
-423.608428	-4.286280	7.745075
-421.716896	1.627889	7.755072
-419.340675	-0.169272	7.765069
-417.633465	-5.292117	7.775066
-416.071940	-6.534468	7.785062
-414.223181	4.312677	7.795059
-411.936233	-4.161564	7.805056
-410.092748	0.062978	7.815053
-408.571823	-2.023908	7.825050
-406.610549	5.172251	7.835046
-404.623723	1.883648	7.845043
-402.889178	0.984719	7.855040
-400.760078	-4.544938	7.865037
-398.882037	1.488242	7.875034
-397.221434	2.438953	7.885030
-395.279602	3.815273	7.895027
-393.421001	1.429753	7.905024
-391.407675	4.872484	7.915021
-389.538314	4.653068	7.925018
-387.874681	2.421834	7.935014
-385.918338	4.086362	7.945011
-384.051189	-1.238834	7.955008
-382.112188	-9.981167	7.965005
-380.454418	-3.183357	7.975002
-378.501152	-1.589383	7.984998
-376.284839	1.086767	7.994995
-374.685081	0.285164	8.004992
-372.522561	-7.368678	8.014989
-371.054354	-8.583470	8.024986
-369.096351	-6.593943	8.034982
-367.262128	6.464436	8.044979
-364.945117	-2.166140	8.054976
-363.386969	-2.226906	8.064973
-361.652727	-4.278349	8.074970
-359.464823	0.200711	8.084966
-357.800202	-4.165322	8.094963
-355.952560	-5.063326	8.104960
-354.068841	-2.962457	8.114957
-351.978253	-1.635112	8.124954
-350.039348	-4.598662	8.134950
-348.427862	-1.833823	8.144947
-346.561247	-1.850669	8.154944
-344.596914	-6.436639	8.164941
-342.917470	-5.997301	8.174938
-341.067110	0.345072	8.184934
-338.926339	-4.155380	8.194931
-337.011457	-4.754641	8.204928
-335.258661	-7.405848	8.214925
-333.255678	-2.853035	8.224922
-331.499739	-6.510495	8.234918
-329.580641	-2.294801	8.244915
-327.760145	-5.593104	8.254912
-325.917781	-6.425508	8.264909
-324.032513	-3.554362	8.274906
-321.988296	-4.805815	8.284902
-320.279650	-1.567009	8.294899
-318.311539	-2.687892	8.304896
-316.586333	-1.166405	8.314893
-314.693240	2.317690	8.324890
-312.720177	2.408610	8.334886
-310.628521	-0.546137	8.344883
-308.897510	-0.306053	8.354880
-307.162437	-2.506005	8.364877
-304.899984	-7.785300	8.374874
-303.206994	-6.236556	8.384870
-301.903285	-7.213477	8.394867
-299.660204	1.054070	8.404864
-297.517511	-4.090843	8.414861
-295.526828	-14.357099	8.424858
-293.966813	-6.163669	8.434854
-292.446911	-7.077203	8.444851
-290.010901	-3.859744	8.454848
-288.700961	-11.622155	8.464845
-286.443714	-7.297776	8.474842
-284.394360	-4.391212	8.484838
-282.791693	-7.872600	8.494835
-280.844985	-3.912317	8.504832
-278.837674	0.270394	8.514829
-277.065976	-6.517333	8.524826
-275.372366	-7.809096	8.534822
-273.174639	-7.406647	8.544819
-271.411087	-6.642800	8.554816
-269.538624	-5.244253	8.564813
-267.439938	-0.616659	8.574810
-265.835647	-8.694455	8.584807
-264.063433	-4.952614	8.594803
-262.271858	-7.201025	8.604800
-260.136861	-8.335867	8.614797
-257.967676	-8.464093	8.624794
-256.673434	-14.035636	8.634791
-254.636036	-2.113236	8.644787
-252.505211	-5.325230	8.654784
-250.951432	-2.844787	8.664781
-248.789713	-8.603726	8.674778
-246.958789	-8.802688	8.684775
-245.104378	-7.737544	8.694771
-243.399481	0.270177	8.704768
-241.342514	1.265102	8.714765
-239.355960	-7.573138	8.724762
-237.526466	-4.175143	8.734759
-235.725993	-5.850238	8.744755
-233.734004	1.748527	8.754752
-232.071170	-15.864058	8.764749
-230.129816	-7.541975	8.774746
-228.309484	-17.062597	8.784743
-226.471903	-15.863706	8.794739
-224.577235	-10.308284	8.804736
-222.269321	-14.784785	8.814733
-220.687204	-10.510486	8.824730
-218.781134	-13.512902	8.834727
-217.166771	-6.486998	8.844723
-215.595360	-6.759778	8.854720
-213.181522	-10.710038	8.864717
-211.376371	-6.687633	8.874714
-209.251569	-14.425316	8.884711
-207.901769	-15.071660	8.894707
-206.168747	-14.568147	8.904704
-204.045549	-16.064202	8.914701
-201.666428	-18.638429	8.924698
-200.246966	-20.383742	8.934695
-198.490703	-4.614451	8.944691
-196.234338	-13.749915	8.954688
-194.477204	-17.630093	8.964685
-192.551429	-11.852248	8.974682
-190.876294	-11.710527	8.984679
-188.835627	-10.532962	8.994675
-186.973671	-18.411832	9.004672
-185.054582	-10.929287	9.014669
-183.119938	-9.783744	9.024666
-181.672308	-13.390322	9.034663
-179.626348	-11.419410	9.044659
-177.686614	-6.815317	9.054656
-175.575428	-13.958716	9.064653
-173.901655	-6.511220	9.074650
-171.918435	-13.646827	9.084647
-170.188222	-8.159850	9.094643
-168.113371	-15.313232	9.104640
-166.447782	-13.734756	9.114637
-164.537185	-8.884432	9.124634
-162.673870	-10.929490	9.134631
-160.657830	-8.600114	9.144627
-158.819495	-8.318628	9.154624
-156.897630	-13.005041	9.164621
-155.100448	-9.226050	9.174618
-153.440838	-16.753674	9.184615
-151.376496	-8.807976	9.194611
-149.702395	-6.296140	9.204608
-147.698689	-14.442332	9.214605
-145.630083	-9.135642	9.224602
-143.713194	-8.441955	9.234599
-141.872357	-12.817017	9.244595
-140.100842	-5.445089	9.254592
-138.190710	-2.986693	9.264589
-136.258035	-5.169110	9.274586
-134.421863	-4.770422	9.284583
-132.694797	-1.125481	9.294579
-130.904315	-0.196885	9.304576
-128.576462	-1.660795	9.314573
-127.060724	-10.521724	9.324570
-124.924818	-4.750503	9.334567
-123.457503	-4.041910	9.344563
-121.549271	-3.245775	9.354560
-119.564477	-11.559452	9.364557
-117.416097	-3.622390	9.374554
-115.599418	-8.906182	9.384551
-114.002520	-4.174706	9.394547
-111.769828	-9.616445	9.404544
-109.826935	-7.033784	9.414541
-108.487314	-7.888442	9.424538
-106.360621	-9.804957	9.434535
-104.534509	-8.266257	9.444531
-102.547326	-5.068571	9.454528
-100.621791	-9.142917	9.464525
-98.949043	-3.589874	9.474522
-97.183967	-5.227643	9.484519
-94.767258	-2.827927	9.494515
-93.351526	-8.208785	9.504512
-91.395696	-11.299567	9.514509
-89.448282	-6.507157	9.524506
-87.321527	-4.361165	9.534503
-85.805341	-7.032869	9.544499
-83.610933	0.806888	9.554496
-81.843913	-1.004859	9.564493
-80.041216	-4.011207	9.574490
-78.316549	-12.835968	9.584487
-76.461846	-2.420515	9.594483
-74.515633	-2.841416	9.604480
-72.721497	-5.007997	9.614477
-70.517989	-16.763787	9.624474
-68.889146	-0.620374	9.634471
-66.904023	-6.990445	9.644467
-65.142462	-3.876730	9.654464
-63.212282	-4.323484	9.664461
-61.324861	-3.833445	9.674458
-59.304646	-0.535204	9.684455
-57.496355	-0.485683	9.694451
-55.832907	-2.118263	9.704448
-53.772337	-10.682394	9.714445
-51.905489	-7.078640	9.724442
-49.793958	-3.057613	9.734439
-48.189041	-8.023377	9.744435
-46.438695	-7.194102	9.754432
-44.435269	-2.685314	9.764429
-42.627672	2.413645	9.774426
-40.792767	1.814743	9.784423
-38.816718	-1.222386	9.794419
-36.895029	0.725844	9.804416
-34.937744	-0.830440	9.814413
-32.969895	1.317266	9.824410
-31.168281	-1.482039	9.834407
-29.506667	1.399761	9.844403
-27.715018	1.478800	9.854400
-25.632270	3.000309	9.864397
-23.877127	-0.522608	9.874394
-21.673909	1.696508	9.884391
-19.992598	3.187321	9.894387
-18.269609	-5.585037	9.904384
-16.270443	-9.945793	9.914381
-14.189734	-6.289281	9.924378
-12.501917	-13.279760	9.934375
-10.945164	-13.412707	9.944371
-8.800051	-3.954540	9.954368
-6.771125	-11.392571	9.964365
-5.032922	-10.992368	9.974362
-3.726059	16.058979	9.984359
-2.574249	45.726090	9.994355
-1.403444	110.550955	10.004352
0.000000	151.230040	10.009357
0.150002	195.778782	10.014362
1.259226	224.646881	10.019367
1.637829	254.325411	10.024371
1.311568	289.977806	10.029376
2.042322	299.294389	10.034381
2.437836	316.859670	10.039386
2.625692	333.524559	10.044391
3.135517	337.503854	10.049395
2.972496	351.725316	10.054400
3.028259	358.585530	10.059405
3.302992	381.129564	10.064410
3.931784	377.976405	10.069415
3.843608	363.511242	10.074419
3.412148	371.926747	10.079424
3.756135	359.526231	10.084429
3.456656	375.463093	10.089434
3.484392	385.500554	10.094439
3.764064	388.286574	10.099443
3.552577	394.907162	10.104448
3.965321	397.422805	10.109453
3.810439	412.817836	10.114458
3.966452	397.927344	10.119463
3.989413	409.061545	10.124467
4.020275	413.134601	10.129472
4.016044	404.079053	10.134477
3.917313	414.201360	10.139482
4.191919	414.841998	10.144487
4.330600	417.618972	10.149491
4.121992	416.193642	10.154496
4.324654	412.884520	10.159501
3.993205	410.959974	10.164506
4.351322	417.669491	10.169511
4.255482	430.776468	10.174515
4.239943	432.715465	10.179520
4.404770	429.029181	10.184525
4.215710	428.679348	10.189530
4.469137	452.814857	10.194535
4.799449	456.226738	10.199539
4.796627	459.770601	10.204544
4.805540	459.039113	10.209549
4.558319	465.777395	10.214554
4.812884	462.407945	10.219559
4.951002	459.900726	10.224563
4.555073	464.814565	10.229568
4.909161	466.581072	10.234573
4.903148	472.503458	10.239578
5.281123	470.000558	10.244583
5.378393	467.995009	10.249587
5.054769	470.170804	10.254592
5.374329	484.965122	10.259597
5.354103	475.588809	10.264602
5.346738	473.737141	10.269607
4.935049	482.884407	10.274611
5.167636	485.804110	10.279616
5.238104	482.664289	10.284621
5.154066	484.027599	10.289626
5.128722	484.861160	10.294631
5.121538	480.279793	10.299635
5.194886	482.598852	10.304640
5.535444	491.361216	10.309645
5.454490	516.291322	10.314650
5.723900	516.215288	10.319655
5.778510	518.685574	10.324659
5.612415	521.597911	10.329664
5.833972	522.814713	10.334669
5.907181	517.977663	10.339674
5.716649	533.361162	10.344679
5.808666	539.315248	10.349683
5.873558	523.751615	10.354688
5.965990	518.026838	10.359693
5.678591	529.160172	10.364698
5.775192	540.446730	10.369703
6.148510	535.181765	10.374707
5.599732	535.944276	10.379712
6.132553	549.299593	10.384717
6.381529	556.857630	10.389722
6.452870	558.535207	10.394727
6.453279	555.953742	10.399731
6.518012	563.959059	10.404736
6.829226	548.431805	10.409741
6.720326	546.946403	10.414746
6.560050	545.951739	10.419751
6.729794	545.869525	10.424755
6.154042	542.069523	10.429760
6.521992	552.306724	10.434765
6.561745	563.782139	10.439770
6.758183	564.998220	10.444775
6.776902	570.282771	10.449779
6.595864	577.417399	10.454784
7.019070	565.324192	10.459789
6.945959	579.597769	10.464794
6.713948	570.650986	10.469799
7.198400	575.036515	10.474803
7.120136	583.611849	10.479808
7.112007	560.816925	10.484813
7.248252	580.797176	10.489818
7.565911	575.151570	10.494823
7.158223	579.452315	10.499827
7.117578	570.318893	10.504832
7.361362	568.558042	10.509837
7.353922	570.503650	10.514842
7.058801	577.369471	10.519847
7.410708	572.628299	10.524851
7.197805	578.930655	10.529856
7.402964	587.807713	10.534861
7.777203	598.343563	10.539866
7.955239	596.749313	10.544871
8.095462	591.057885	10.549875
8.106528	590.748668	10.554880
8.034086	575.766699	10.559885
7.700429	585.768902	10.564890
7.989494	580.474782	10.569895
7.970671	580.022100	10.574899
7.758451	571.781784	10.579904
8.016695	572.669465	10.584909
8.113507	581.185335	10.589914
8.561566	581.784124	10.594919
8.380909	585.883081	10.599923
7.992439	583.163365	10.604928
8.361816	578.966604	10.609933
8.102463	588.116446	10.614938
8.014704	584.065135	10.619943
8.082523	588.622776	10.624947
8.425794	590.830992	10.629952
8.672926	609.785930	10.634957
8.402538	600.045738	10.639962
8.751104	585.638426	10.644967
8.575816	592.652297	10.649971
8.228519	601.216935	10.654976
8.657143	603.023611	10.659981
8.560861	621.708487	10.664986
8.623864	620.058465	10.669991
9.056970	615.075672	10.674995
8.579300	618.584924	10.680000
8.926061	629.013216	10.685005
8.912615	624.096913	10.690010
8.967551	627.302022	10.695015
8.905457	616.287539	10.700019
8.816370	631.435766	10.705024
9.013057	618.774673	10.710029
9.054349	616.869495	10.715034
8.890653	629.648431	10.720039
9.199501	626.308132	10.725043
9.492916	623.023912	10.730048
9.331309	620.357891	10.735053
8.980457	631.849929	10.740058
9.270979	625.581006	10.745063
9.423650	635.411058	10.750067
9.371825	650.581747	10.755072
9.780768	649.062626	10.760077
9.807159	666.051695	10.765082
9.799665	649.660534	10.770087
9.676541	643.938549	10.775091
9.719817	640.255829	10.780096
10.037266	633.709796	10.785101
9.499838	641.806468	10.790106
9.955286	642.268463	10.795111
9.866421	655.852347	10.800115
10.020253	656.556415	10.805120
10.074040	663.959560	10.810125
10.168013	654.676880	10.815130
9.894307	657.327288	10.820135
9.947496	650.903820	10.825139
9.994168	664.175935	10.830144
10.136731	657.397588	10.835149
10.125790	668.330815	10.840154
10.112911	661.328101	10.845159
10.126235	662.508741	10.850163
10.372511	670.485161	10.855168
10.446440	652.283285	10.860173
10.206923	668.206172	10.865178
10.296516	653.281857	10.870183
10.494976	663.721212	10.875187
10.345566	662.218605	10.880192
10.477072	662.371148	10.885197
10.788073	681.558844	10.890202
10.831847	678.350698	10.895207
10.912623	679.241461	10.900211
10.435902	676.389146	10.905216
10.921725	683.630353	10.910221
10.788314	691.036562	10.915226
11.180871	692.251336	10.920231
11.228949	693.571516	10.925235
11.110462	704.149762	10.930240
11.437535	679.344185	10.935245
11.058204	671.357547	10.940250
11.356259	653.682893	10.945255
11.468792	661.710602	10.950259
11.217630	662.122874	10.955264
11.352738	667.869868	10.960269
11.547358	659.574074	10.965274
11.107167	656.624473	10.970279
11.279846	661.925502	10.975283
11.204228	673.854644	10.980288
11.396185	674.505324	10.985293
11.404802	691.412103	10.990298
11.316720	707.492230	10.995303
11.792513	695.554531	11.000307
11.709881	699.693079	11.005312
11.963202	706.824724	11.010317
11.618679	703.806238	11.015322
11.712501	692.298473	11.020327
11.378383	698.071433	11.025331
11.560240	712.798061	11.030336
11.666450	693.570693	11.035341
11.686009	693.898786	11.040346
11.965308	704.643822	11.045351
12.106177	717.626572	11.050355
11.977772	727.268127	11.055360
12.389057	717.302437	11.060365
12.309324	723.187798	11.065370
12.525309	721.812987	11.070375
12.363730	725.238732	11.075379
12.237401	726.823276	11.080384
12.514291	726.485851	11.085389
12.387299	722.937501	11.090394
12.281987	722.146947	11.095399
12.389811	728.716758	11.100403
12.391239	725.819709	11.105408
12.543395	719.244808	11.110413
12.492716	728.995393	11.115418
12.624610	719.968398	11.120423
12.895255	716.815523	11.125427
12.531755	730.268237	11.130432
12.926582	723.138963	11.135437
12.608399	725.637204	11.140442
12.966088	729.347561	11.145447
12.705734	727.720716	11.150451
12.440768	733.083689	11.155456
13.218639	743.552115	11.160461
13.318740	753.228205	11.165466
13.334284	744.905730	11.170471
13.271118	730.600214	11.175475
12.710829	737.707100	11.180480
13.284678	745.424734	11.185485
13.793394	747.464661	11.190490
13.684034	746.666867	11.195495
13.582353	725.640184	11.200499
13.057260	723.620323	11.205504
13.156900	721.716864	11.210509
13.315985	748.848367	11.215514
13.637018	746.707742	11.220519
13.878347	747.456207	11.225523
13.814427	750.254522	11.230528
14.299463	745.200324	11.235533
14.117092	737.149118	11.240538
13.690198	730.001091	11.245543
13.829715	722.933039	11.250547
13.868181	725.311317	11.255552
14.143241	717.928335	11.260557
13.938862	721.122785	11.265562
13.895046	721.700685	11.270567
14.022132	734.695110	11.275571
14.239776	744.317753	11.280576
14.271078	729.311193	11.285581
14.006965	733.376193	11.290586
14.200435	746.473582	11.295591
14.485300	751.248970	11.300595
14.206765	766.113738	11.305600
14.226465	753.950691	11.310605
14.140577	755.653368	11.315610
14.289507	756.424456	11.320615
14.624854	753.474143	11.325619
14.251713	758.196785	11.330624
14.342878	758.084526	11.335629
14.066039	764.241039	11.340634
14.203945	769.437267	11.345639
14.696264	776.680640	11.350643
14.782697	780.054226	11.355648
15.076284	769.161094	11.360653
15.069072	775.672003	11.365658
15.017391	764.837097	11.370663
15.164255	755.233678	11.375667
14.713276	758.787591	11.380672
14.999428	760.386775	11.385677
14.790934	762.444901	11.390682
15.240346	773.307938	11.395687
14.885323	791.097584	11.400691
15.219679	785.966479	11.405696
15.724922	783.455845	11.410701
15.461618	793.658281	11.415706
15.286313	783.494365	11.420711
15.520744	775.053383	11.425715
15.254094	781.730254	11.430720
15.983241	776.413182	11.435725
15.710523	775.091080	11.440730
15.593643	768.494411	11.445735
15.555721	752.775042	11.450739
15.354432	761.106750	11.455744
15.817265	767.599456	11.460749
15.805458	766.338244	11.465754
15.487420	763.695569	11.470759
15.765033	763.499955	11.475763
15.948439	793.079839	11.480768
16.223357	789.602989	11.485773
15.930564	800.278492	11.490778
16.070466	781.580225	11.495783
16.151501	782.083020	11.500787
16.076556	789.304910	11.505792
16.191121	781.982187	11.510797
16.058286	786.053072	11.515802
15.863291	787.301641	11.520807
16.246906	798.403852	11.525811
16.070074	786.868216	11.530816
16.123855	796.740959	11.535821
15.966514	780.230045	11.540826
16.302260	791.415579	11.545831
16.570014	786.515872	11.550835
16.358777	787.815918	11.555840
16.409349	792.726461	11.560845
16.238631	790.345714	11.565850
16.209843	800.078663	11.570855
16.634504	820.208789	11.575859
16.736323	819.919786	11.580864
16.904590	824.549791	11.585869
17.103603	823.117753	11.590874
16.598003	821.011189	11.595879
17.194457	815.379373	11.600883
17.238107	819.728051	11.605888
17.213363	813.509331	11.610893
16.999332	827.636892	11.615898
17.398262	822.907065	11.620903
17.344913	808.457978	11.625907
16.924773	787.374764	11.630912
16.617276	804.366787	11.635917
17.092787	806.391518	11.640922
17.193560	822.422728	11.645927
17.360929	813.680180	11.650931
17.151005	826.495047	11.655936
17.666154	815.128146	11.660941
17.846548	819.805101	11.665946
17.650253	823.020361	11.670951
17.672539	813.078802	11.675955
17.627173	824.597962	11.680960
17.590721	820.156775	11.685965
17.551016	819.415676	11.690970
17.929310	821.397568	11.695975
17.905219	816.645324	11.700979
18.051726	828.461895	11.705984
18.462571	802.001122	11.710989
18.329771	820.748850	11.715994
18.152994	805.441081	11.720999
17.871024	786.206114	11.726003
17.693860	798.500064	11.731008
18.014524	811.670267	11.736013
18.072721	803.801431	11.741018
18.024678	816.921634	11.746023
18.162708	819.481169	11.751027
17.867765	813.761288	11.756032
18.201280	809.917116	11.761037
18.255766	816.266814	11.766042
18.299963	818.560614	11.771047
18.219627	815.529930	11.776051
18.405918	818.640014	11.781056
18.500372	812.321859	11.786061
18.428286	815.209798	11.791066
18.427679	814.169148	11.796071
18.636824	826.857252	11.801075
18.923418	831.484157	11.806080
19.067509	831.000752	11.811085
18.746234	833.250342	11.816090
18.573059	834.586900	11.821095
18.923884	837.670747	11.826099
19.101393	847.949573	11.831104
18.963189	834.363982	11.836109
18.907468	850.522686	11.841114
18.959593	850.626390	11.846119
19.259262	842.812060	11.851123
19.034731	838.460789	11.856128
19.255094	846.433556	11.861133
19.345798	835.973284	11.866138
19.309302	840.192823	11.871143
19.171267	838.630035	11.876147
19.064804	842.032824	11.881152
19.175013	836.401282	11.886157
19.262860	827.814912	11.891162
18.978719	835.194771	11.896167
19.066193	835.769082	11.901171
19.232810	856.411930	11.906176
19.758525	859.745435	11.911181
19.945912	862.426418	11.916186
19.798296	864.328190	11.921191
19.887207	856.585314	11.926195
19.889723	868.003831	11.931200
20.310194	841.700725	11.936205
19.998394	844.324124	11.941210
19.890267	830.599697	11.946215
20.114361	821.870174	11.951219
19.897171	828.496599	11.956224
20.012484	827.412228	11.961229
20.125957	836.483839	11.966234
20.234825	848.848908	11.971239
20.108444	840.678326	11.976243
20.094229	861.484065	11.981248
20.282630	856.489757	11.986253
20.127207	868.991613	11.991258
20.092844	858.928168	11.996263
20.363807	856.544776	12.001267
20.289865	864.700112	12.006272
20.375630	860.496466	12.011277
20.445274	857.388235	12.016282
20.290270	866.799156	12.021287
20.521592	860.626309	12.026291
20.312192	860.361711	12.031296
20.520462	849.822753	12.036301
20.365874	859.831275	12.041306
20.570283	869.877166	12.046311
20.644301	861.370254	12.051315
20.435315	862.931725	12.056320
20.642265	860.533310	12.061325
20.477149	860.706355	12.066330
20.653278	857.115934	12.071335
20.600524	865.094424	12.076339
20.754393	868.217575	12.081344
20.972470	863.694778	12.086349
20.756705	862.021380	12.091354
20.708201	853.735867	12.096359
21.025421	853.715287	12.101363
20.661355	853.256158	12.106368
20.497414	825.863560	12.111373
20.585935	830.991993	12.116378
20.593093	830.464195	12.121383
20.648642	815.559335	12.126387
20.597879	835.254372	12.131392
20.766225	817.671170	12.136397
20.688216	830.759895	12.141402
20.528962	824.507430	12.146407
20.570216	825.120652	12.151411
20.612095	826.014474	12.156416
20.652180	828.400396	12.161421
20.350472	834.150893	12.166426
20.373373	822.050356	12.171431
20.432282	827.839530	12.176435
20.309036	832.109173	12.181440
20.726495	836.158537	12.186445
20.655914	829.396758	12.191450
20.631268	831.624269	12.196455
20.945316	826.587854	12.201459
20.796864	833.438287	12.206464
20.748786	823.279282	12.211469
20.850622	816.829058	12.216474
20.689692	811.887327	12.221479
20.824418	810.861362	12.226483
20.490759	810.993479	12.231488
20.501691	804.748572	12.236493
20.595137	799.958664	12.241498
20.553455	814.490813	12.246503
20.661540	804.712195	12.251507
20.654631	807.080378	12.256512
21.093697	807.863542	12.261517
20.814625	803.874221	12.266522
20.595215	813.863088	12.271527
20.756998	800.083025	12.276531
20.494724	790.290946	12.281536
20.379376	780.137969	12.286541
20.439426	786.655502	12.291546
20.419325	796.730842	12.296551
20.346456	797.120988	12.301555
20.355843	800.584139	12.306560
20.658918	815.856095	12.311565
20.485131	811.976137	12.316570
20.381035	824.069219	12.321575
20.407125	814.503947	12.326579
20.170082	819.283750	12.331584
20.446048	815.459794	12.336589
20.555578	816.998845	12.341594
20.039307	810.166232	12.346599
20.414400	818.235732	12.351603
20.468761	811.269529	12.356608
20.430750	809.189315	12.361613
20.336912	810.651990	12.366618
20.324848	819.601686	12.371623
20.728493	817.566148	12.376627
20.344762	817.433435	12.381632
20.622163	810.209307	12.386637
20.514756	826.090797	12.391642
20.238152	822.047460	12.396647
20.243097	815.049712	12.401651
20.529715	823.328870	12.406656
20.676188	816.783217	12.411661
20.646152	821.037991	12.416666
20.573646	824.561518	12.421671
20.511051	815.522905	12.426675
20.447930	826.929781	12.431680
20.528224	819.964169	12.436685
20.648902	826.714903	12.441690
20.494520	824.132847	12.446695
20.831874	816.937001	12.451699
20.383857	820.883121	12.456704
20.704923	810.124349	12.461709
20.310709	825.874961	12.466714
20.323184	823.431875	12.471719
20.686861	819.328997	12.476723
20.524345	818.019277	12.481728
20.577330	825.416326	12.486733
20.717811	821.809521	12.491738
20.677705	821.675619	12.496743
20.698008	834.385965	12.501747
20.558015	822.281446	12.506752
20.686939	830.044858	12.511757
20.920137	824.713829	12.516762
20.514762	822.993406	12.521767
20.648796	792.315828	12.526771
20.639600	798.148969	12.531776
20.523961	787.210704	12.536781
20.594766	789.709993	12.541786
20.487156	794.849194	12.546791
20.737709	795.148332	12.551795
20.591681	797.098728	12.556800
20.574950	798.385099	12.561805
20.589041	794.721188	12.566810
20.249370	801.507485	12.571815
20.583769	796.332215	12.576819
20.032008	800.294876	12.581824
20.252281	793.671230	12.586829
20.439938	792.259930	12.591834
20.339132	799.367678	12.596839
20.854169	786.960019	12.601843
20.528745	786.893701	12.606848
20.756146	797.714896	12.611853
20.632041	782.411365	12.616858
20.151612	791.263854	12.621863
20.979264	791.455180	12.626867
20.579109	796.560615	12.631872
20.200034	800.424770	12.636877
20.120776	790.847931	12.641882
20.061955	805.562579	12.646887
20.221434	796.501174	12.651891
20.318373	824.484832	12.656896
20.566037	816.882240	12.661901
20.325261	831.001455	12.666906
20.507247	833.271704	12.671911
20.793524	824.877618	12.676915
20.491797	835.568765	12.681920
20.479987	823.259295	12.686925
20.357155	834.270419	12.691930
20.669538	834.211187	12.696935
20.641091	822.550929	12.701939
20.625890	817.835114	12.706944
20.358264	816.152647	12.711949
20.293617	812.679486	12.716954
20.203664	829.130635	12.721959
20.682983	824.178249	12.726963
20.342985	836.370467	12.731968
20.388001	843.563790	12.736973
20.591703	836.261516	12.741978
20.354039	841.982877	12.746983
20.506473	836.227905	12.751987
20.364013	851.192484	12.756992
20.788216	835.199043	12.761997
20.856042	842.213684	12.767002
20.765885	839.326488	12.772007
20.761826	811.589869	12.777011
20.468808	812.768918	12.782016
20.182720	810.816580	12.787021
20.324749	813.459056	12.792026
20.558354	825.930368	12.797031
20.874511	818.923984	12.802035
20.655328	815.062305	12.807040
20.391759	806.003712	12.812045
20.576158	815.669553	12.817050
20.577024	807.485002	12.822055
20.402753	808.022210	12.827059
20.222968	819.371992	12.832064
20.431646	816.809304	12.837069
20.552566	808.457370	12.842074
20.511648	815.692770	12.847079
20.825419	804.935166	12.852083
20.430122	810.047715	12.857088
20.646570	805.536234	12.862093
20.681738	800.635771	12.867098
20.426588	809.520151	12.872103
20.664654	809.092723	12.877107
20.873731	810.838248	12.882112
20.843144	799.965257	12.887117
20.490594	810.300212	12.892122
20.497160	808.214465	12.897127
20.859372	806.332196	12.902131
20.522204	809.325492	12.907136
20.609065	802.234260	12.912141
20.620198	809.191694	12.917146
20.745053	807.158045	12.922151
20.968955	797.493425	12.927155
20.465189	787.673631	12.932160
20.232312	782.459531	12.937165
20.360659	777.589946	12.942170
20.470646	789.486427	12.947175
20.607970	790.663072	12.952179
20.114358	801.070981	12.957184
20.445851	799.070608	12.962189
20.724642	811.842210	12.967194
20.483032	812.489507	12.972199
20.723763	815.392210	12.977203
20.465398	802.133323	12.982208
20.193613	799.383914	12.987213
20.490988	799.961016	12.992218
20.458904	817.140942	12.997223
20.817787	809.252531	13.002227
20.487923	813.457350	13.007232
20.696638	813.296380	13.012237
20.341386	789.660739	13.017242
20.216407	802.697005	13.022247
20.749434	797.411207	13.027251
20.453917	809.744544	13.032256
20.587476	798.206702	13.037261
20.330339	799.050442	13.042266
20.200923	813.897784	13.047271
20.188191	814.037063	13.052275
20.372404	823.983640	13.057280
20.530822	818.986241	13.062285
20.801168	818.766555	13.067290
20.505668	823.707072	13.072295
20.529314	825.212513	13.077299
20.471351	828.803108	13.082304
20.576979	825.203438	13.087309
20.800985	827.659375	13.092314
20.710154	828.249508	13.097319
20.757308	802.732996	13.102323
20.487239	793.699102	13.107328
20.380055	793.281007	13.112333
20.549384	795.081756	13.117338
20.301029	796.125946	13.122343
20.461451	788.092579	13.127347
20.344597	796.185335	13.132352
20.443225	798.278060	13.137357
20.705003	804.900624	13.142362
20.589082	812.807157	13.147367
20.489593	797.045518	13.152371
20.431964	800.129847	13.157376
20.191027	804.670568	13.162381
20.787800	799.808268	13.167386
20.642072	804.988245	13.172391
20.798345	789.733030	13.177395
20.632967	811.177823	13.182400
20.618364	783.453978	13.187405
20.750962	799.158386	13.192410
20.401359	798.890919	13.197415
20.663189	791.926328	13.202419
20.735014	803.932988	13.207424
20.813100	800.314062	13.212429
20.856253	795.593678	13.217434
20.459467	800.506187	13.222439
20.626801	799.191169	13.227443
20.391069	797.073105	13.232448
20.478606	791.412080	13.237453
20.784405	789.049950	13.242458
20.571441	804.006803	13.247463
20.584138	803.683128	13.252467
20.495147	791.661965	13.257472
20.611782	791.031552	13.262477
20.929876	778.634809	13.267482
20.516696	775.233016	13.272487
20.649312	758.983387	13.277491
20.181063	772.713046	13.282496
20.452154	765.223439	13.287501
20.631974	763.408112	13.292506
19.995628	772.738047	13.297511
20.650371	768.449988	13.302515
20.244633	779.559808	13.307520
20.128684	792.421159	13.312525
20.493963	796.942462	13.317530
20.460693	806.097383	13.322535
20.445468	795.278716	13.327539
20.646353	804.524025	13.332544
20.493130	803.868842	13.337549
20.599252	793.380909	13.342554
20.434305	811.717435	13.347559
20.823922	805.150354	13.352563
20.598814	809.037264	13.357568
20.626601	799.356613	13.362573
20.462120	782.605558	13.367578
20.410345	782.959223	13.372583
20.152807	781.956400	13.377587
20.103553	795.682332	13.382592
20.448211	797.064030	13.387597
20.694977	799.418561	13.392602
20.359539	804.702912	13.397607
20.517851	801.093269	13.402611
20.580805	803.209032	13.407616
20.606870	803.506127	13.412621
20.817568	807.706732	13.417626
20.737644	804.049928	13.422631
20.707767	788.417546	13.427635
20.514908	782.736590	13.432640
20.425372	772.768737	13.437645
20.124208	766.644587	13.442650
20.055993	793.137487	13.447655
20.461742	789.139872	13.452659
20.181052	808.480457	13.457664
20.623758	795.149185	13.462669
20.508908	805.116639	13.467674
20.780699	807.620145	13.472679
20.590371	799.332051	13.477683
20.349012	815.562902	13.482688
20.699945	808.667672	13.487693
20.782036	812.486664	13.492698
20.506398	798.383703	13.497703
20.648761	800.521494	13.502707
20.476049	782.734107	13.507712
20.284385	777.697941	13.512717
20.396229	796.605317	13.517722
20.596423	800.758710	13.522727
20.626139	802.890813	13.527731
20.360950	804.883869	13.532736
20.433550	798.523473	13.537741
20.584662	799.683726	13.542746
20.326188	806.237877	13.547751
20.341779	792.933727	13.552755
20.509874	811.338561	13.557760
20.432592	802.452111	13.562765
20.736883	812.196600	13.567770
20.538702	805.983468	13.572775
20.908819	800.720497	13.577779
20.626928	796.091379	13.582784
20.435856	788.930941	13.587789
20.362490	771.654430	13.592794
20.309681	790.766256	13.597799
20.518178	784.795780	13.602803
20.682158	793.472952	13.607808
20.589869	790.131940	13.612813
20.232613	774.446131	13.617818
20.299619	793.753319	13.622823
20.769954	793.817129	13.627827
20.385478	802.181231	13.632832
20.433393	791.475501	13.637837
20.481370	799.092533	13.642842
20.555385	807.780909	13.647847
20.736031	789.979734	13.652851
20.564793	794.517220	13.657856
20.219745	787.348224	13.662861
20.308447	786.061518	13.667866
20.078972	810.074370	13.672871
20.724808	803.319767	13.677875
20.912051	811.133793	13.682880
20.540311	808.796143	13.687885
20.343177	804.680212	13.692890
20.458986	806.528923	13.697895
20.640071	801.568917	13.702899
20.526657	794.626327	13.707904
20.314035	793.103825	13.712909
20.449051	797.776972	13.717914
20.300588	813.240791	13.722919
20.606018	813.890726	13.727923
20.417585	824.835034	13.732928
20.598807	814.756159	13.737933
21.035709	822.500410	13.742938
20.372092	806.838196	13.747943
20.728003	785.031962	13.752947
20.368664	799.515411	13.757952
20.566136	788.145581	13.762957
20.549471	786.877257	13.767962
20.262902	795.476478	13.772967
20.571073	778.467116	13.777971
20.498898	793.768935	13.782976
20.538679	784.333965	13.787981
20.467624	780.746716	13.792986
20.715683	792.192243	13.797991
20.735098	791.514258	13.802995
20.463351	794.847203	13.808000
20.420398	790.430715	13.813005
20.578204	794.955146	13.818010
20.311514	794.310176	13.823015
20.789635	791.173080	13.828019
20.755837	781.481763	13.833024
20.834524	786.774176	13.838029
20.689724	788.092011	13.843034
20.836633	795.620722	13.848039
20.693583	793.058942	13.853043
20.755458	786.987269	13.858048
20.726488	794.539300	13.863053
20.850220	790.522009	13.868058
20.571929	780.439175	13.873063
20.293209	771.007703	13.878067
20.307652	766.810729	13.883072
20.249186	778.530640	13.888077
20.492459	777.580406	13.893082
20.832792	781.834445	13.898087
20.805555	784.303638	13.903091
20.027527	783.591988	13.908096
20.476666	764.196289	13.913101
20.573201	769.462194	13.918106
20.277686	771.969442	13.923111
20.587240	766.372365	13.928115
20.560676	798.519931	13.933120
20.448353	785.012260	13.938125
20.697135	791.679469	13.943130
20.117766	790.809976	13.948135
20.443913	793.225962	13.953139
20.659542	798.550155	13.958144
20.549419	787.849132	13.963149
20.636209	789.461194	13.968154
20.158351	795.646627	13.973159
20.334197	777.748461	13.978163
20.353459	789.580564	13.983168
20.218860	792.634589	13.988173
20.477099	799.705572	13.993178
20.548622	801.118218	13.998183
20.725936	783.453202	14.003187
20.651301	802.481792	14.008192
20.116374	801.742846	14.013210
20.511641	791.249667	14.018227
20.467673	806.923253	14.023245
20.333610	801.105918	14.028263
20.638455	799.014095	14.033280
20.768769	798.032295	14.038298
20.664426	803.524407	14.043315
20.239374	800.122337	14.048333
20.461383	803.509707	14.053351
20.435611	798.961770	14.058368
20.467190	798.154584	14.063386
20.771400	799.474578	14.068403
20.339015	810.857783	14.073421
20.559433	797.057843	14.078439
20.265642	804.216033	14.083456
20.211003	809.111939	14.088474
20.705099	835.049720	14.093491
20.779115	829.957347	14.098509
21.146091	830.488725	14.103527
20.942017	838.887834	14.108544
20.528892	839.458693	14.113562
20.794890	831.312493	14.118579
20.529766	830.554201	14.123597
20.595919	842.274748	14.128615
20.758114	835.856469	14.133632
20.776187	829.791499	14.138650
20.985554	832.737322	14.143667
20.849519	818.884107	14.148685
21.170074	829.735126	14.153703
20.697621	829.562005	14.158720
20.668749	830.936700	14.163738
20.955594	836.522155	14.168755
20.821115	857.054911	14.173773
21.176132	867.131289	14.178791
21.367113	858.742221	14.183808
21.272964	869.610651	14.188826
21.356480	862.372818	14.193843
20.955797	855.114693	14.198861
21.307748	853.916650	14.203879
21.131146	858.659000	14.208896
20.723567	869.198338	14.213914
21.232997	864.557155	14.218931
21.384429	876.896455	14.223949
21.168908	875.692967	14.228967
21.290869	870.221717	14.233984
21.230595	862.832220	14.239002
21.278667	863.980724	14.244019
21.455262	872.490591	14.249037
21.409694	863.642195	14.254055
21.470253	871.591722	14.259072
21.115137	871.228434	14.264090
21.439974	865.794038	14.269107
20.803896	875.926252	14.274125
21.097048	863.382449	14.279143
21.532560	867.854150	14.284160
21.333129	875.341802	14.289178
21.318325	859.075180	14.294195
21.442591	878.281598	14.299213
21.761349	860.012887	14.304231
21.795711	864.786083	14.309248
21.387686	878.447807	14.314266
21.726924	865.893506	14.319283
21.561844	864.200651	14.324301
21.217400	872.164439	14.329319
21.446962	873.908460	14.334336
21.702133	889.518695	14.339354
21.857401	889.923400	14.344371
21.996271	904.150698	14.349389
21.802129	874.227958	14.354407
21.787436	871.265339	14.359424
21.515498	873.479437	14.364442
21.678584	864.487655	14.369459
21.757952	895.380422	14.374477
21.949790	895.493017	14.379495
21.998687	892.941804	14.384512
21.747528	877.145421	14.389530
21.973575	876.867186	14.394547
22.017438	892.967283	14.399565
22.231865	872.327453	14.404583
21.987754	871.570525	14.409600
21.717309	872.746236	14.414618
22.071668	856.880040	14.419635
21.877461	862.573689	14.424653
21.893342	859.829555	14.429671
22.145083	880.638930	14.434688
22.138346	890.117100	14.439706
22.254009	884.390457	14.444723
21.919946	885.197234	14.449741
21.982549	870.453457	14.454759
22.635213	887.634590	14.459776
22.001317	873.629503	14.464794
22.139669	865.369942	14.469811
22.153200	873.536174	14.474829
22.099503	870.880210	14.479847
22.547991	883.867383	14.484864
22.235573	877.598712	14.489882
22.325480	861.903671	14.494899
22.336545	860.332154	14.499917
22.179848	853.286787	14.504935
22.505233	869.072983	14.509952
22.082186	873.647014	14.514970
22.457487	875.043763	14.519987
22.490785	883.878498	14.525005
22.254572	880.954354	14.530023
22.323236	887.647381	14.535040
22.175892	895.825126	14.540058
22.508300	881.373345	14.545075
22.436750	892.294814	14.550093
22.571871	887.707031	14.555111
22.754349	888.528947	14.560128
22.285834	897.078800	14.565146
22.508997	880.351076	14.570163
22.647394	883.047118	14.575181
22.661713	899.817294	14.580199
22.763138	876.471123	14.585216
22.668174	888.571318	14.590234
22.945417	882.990357	14.595251
22.666408	891.016075	14.600269
22.800803	880.179065	14.605287
22.850500	877.641884	14.610304
22.671347	881.346499	14.615322
22.762069	871.766959	14.620339
23.080261	878.855893	14.625357
23.074374	861.326338	14.630375
22.905240	860.875189	14.635392
22.574828	861.045910	14.640410
22.623949	860.605567	14.645427
22.723859	867.724590	14.650445
22.758963	877.498085	14.655463
23.275323	879.515674	14.660480
22.997390	882.234074	14.665498
23.180348	867.633118	14.670515
23.155104	852.484964	14.675533
22.575470	857.920773	14.680551
22.898630	861.156751	14.685568
22.987513	884.983860	14.690586
23.223447	873.403956	14.695603
23.154301	888.029341	14.700621
22.932721	891.102107	14.705639
23.228326	885.872131	14.710656
22.875250	886.087364	14.715674
22.976618	892.221497	14.720691
23.147929	889.142697	14.725709
23.073562	888.409030	14.730727
22.794076	887.357309	14.735744
23.026861	891.570355	14.740762
23.322260	892.776938	14.745779
23.347286	893.325106	14.750797
23.161132	885.590748	14.755815
23.425606	887.110562	14.760832
23.052461	904.258704	14.765850
23.178729	888.589294	14.770867
22.964913	897.045044	14.775885
23.270901	893.230641	14.780903
23.801595	896.804744	14.785920
23.286763	904.485853	14.790938
23.524567	886.398326	14.795955
23.650324	900.899834	14.800973
23.605262	886.383988	14.805991
23.742460	877.426213	14.811008
23.351653	888.263323	14.816026
23.438691	890.388711	14.821043
23.409464	887.401667	14.826061
23.225978	892.771161	14.831079
23.413782	901.449137	14.836096
23.413553	902.292329	14.841114
23.834972	914.656239	14.846131
23.622911	910.653907	14.851149
23.656497	916.605388	14.856167
23.770438	908.590359	14.861184
23.922013	920.718898	14.866202
23.867830	910.223388	14.871219
23.725328	924.534907	14.876237
23.950372	902.510710	14.881255
24.139986	907.222981	14.886272
23.686686	911.084581	14.891290
24.006193	902.711167	14.896307
24.112643	910.945967	14.901325
23.711976	908.549818	14.906343
23.884938	904.196657	14.911360
24.022355	912.055301	14.916378
23.923594	916.434486	14.921395
23.990632	915.794663	14.926413
23.928234	914.071269	14.931431
23.915654	909.132673	14.936448
23.613674	906.640565	14.941466
23.790186	905.481510	14.946483
24.005977	903.600496	14.951501
24.071602	917.348728	14.956519
24.417592	912.945946	14.961536
24.398482	900.753922	14.966554
24.245029	899.811081	14.971571
24.257973	906.417053	14.976589
24.375886	902.184352	14.981607
24.652855	901.923163	14.986624
24.264852	895.034211	14.991642
24.264162	891.677689	14.996659
24.376685	898.060146	15.001677
24.028879	895.183683	15.006695
24.465127	907.129961	15.011712
24.327032	904.965630	15.016730
24.353186	897.680302	15.021747
24.382583	897.729146	15.026765
24.188090	903.852273	15.031783
24.466963	903.156644	15.036800
24.337991	907.990510	15.041818
24.203938	897.252929	15.046835
24.481892	893.049759	15.051853
24.344641	909.203928	15.056871
24.836003	906.236093	15.061888
24.608562	910.835565	15.066906
24.311402	915.735581	15.071923
24.776655	919.257209	15.076941
24.911211	927.776960	15.081959
24.819076	907.418771	15.086976
24.613216	911.165404	15.091994
24.753769	894.677345	15.097011
24.780746	906.967311	15.102029
24.615496	909.200576	15.107047
24.932723	917.760396	15.112064
24.909060	924.713547	15.117082
24.678273	920.909246	15.122099
25.022889	928.388802	15.127117
25.029291	922.860460	15.132135
25.312725	920.155437	15.137152
25.107431	904.671018	15.142170
24.807631	897.646880	15.147187
24.897835	901.102484	15.152205
24.979602	907.541758	15.157223
24.972931	894.874295	15.162240
25.035651	895.877326	15.167258
24.598029	905.375467	15.172275
25.059149	905.361747	15.177293
25.049134	925.931377	15.182311
25.444671	934.650170	15.187328
25.246281	925.852850	15.192346
25.013010	913.562842	15.197363
25.234382	909.352962	15.202381
25.294024	934.617779	15.207399
25.532737	913.934692	15.212416
25.404417	903.081367	15.217434
25.087061	900.609014	15.222451
25.134095	895.983370	15.227469
25.310105	917.635398	15.232487
25.701275	925.621884	15.237504
25.570884	921.581356	15.242522
25.129237	905.329279	15.247539
25.315397	893.230359	15.252557
25.241544	916.212057	15.257575
25.159554	918.450920	15.262592
25.304962	915.429725	15.267610
25.270216	930.601774	15.272627
25.461973	929.619604	15.277645
25.220599	936.955107	15.282663
25.596729	933.434661	15.287680
25.308788	931.712632	15.292698
25.507951	934.207091	15.297715
25.837876	923.529192	15.302733
25.276469	939.299604	15.307751
25.376352	939.113846	15.312768
25.825503	942.540525	15.317786
25.659985	952.528532	15.322803
25.770327	946.294647	15.327821
25.765772	947.567950	15.332839
25.940924	955.823277	15.337856
25.819170	943.595679	15.342874
26.074065	946.163046	15.347891
26.085210	930.997995	15.352909
26.170061	926.643150	15.357927
26.118022	928.820611	15.362944
26.144825	920.552070	15.367962
26.145517	921.225237	15.372979
26.221894	919.909127	15.377997
25.990234	921.099104	15.383015
25.904457	927.851387	15.388032
26.072453	920.003901	15.393050
25.872535	924.543934	15.398067
26.015610	916.483356	15.403085
25.914718	916.740162	15.408103
26.053226	924.173940	15.413120
25.937930	927.882540	15.418138
25.719228	925.362989	15.423155
26.109923	934.071544	15.428173
26.126429	958.553658	15.433191
26.320825	949.899735	15.438208
26.626510	941.657486	15.443226
26.449139	948.779875	15.448243
26.706708	942.398247	15.453261
26.453262	931.277005	15.458279
26.327912	925.722486	15.463296
26.533160	927.572634	15.468314
26.521793	928.143910	15.473331
26.443222	914.179196	15.478349
26.167357	926.003121	15.483367
26.436181	920.940992	15.488384
26.580178	942.105826	15.493402
26.458292	944.775755	15.498419
26.720181	944.096990	15.503437
26.268064	946.152653	15.508455
26.522270	954.665920	15.513472
26.846980	946.994764	15.518490
26.779786	942.738094	15.523507
26.911799	946.539383	15.528525
26.541734	955.331533	15.533543
26.835950	939.970322	15.538560
26.661073	933.514529	15.543578
26.954393	956.255267	15.548595
26.975078	952.358943	15.553613
26.914332	955.480000	15.558631
26.776740	952.549549	15.563648
26.722215	948.695107	15.568666
26.636064	952.337719	15.573683
26.856172	958.622823	15.578701
26.618350	954.448416	15.583719
27.005211	946.923071	15.588736
26.759775	957.960408	15.593754
26.728168	957.352046	15.598771
26.911593	951.848941	15.603789
26.673177	951.025035	15.608807
26.872344	949.843489	15.613824
26.872679	963.304888	15.618842
27.208010	971.388392	15.623859
27.509046	964.068628	15.628877
27.474665	981.136090	15.633895
27.280667	957.105478	15.638912
27.383829	949.504260	15.643930
26.917730	954.368315	15.648947
27.215880	973.466907	15.653965
27.239432	982.374040	15.658983
27.542706	966.762828	15.664000
27.730974	969.847319	15.669018
27.019005	963.859402	15.674035
27.404515	960.832937	15.679053
27.432195	979.408408	15.684071
27.446579	972.809158	15.689088
27.659693	976.218437	15.694106
27.559157	968.585206	15.699123
27.456883	966.034496	15.704141
27.771117	960.766917	15.709159
27.716543	964.335285	15.714176
27.608854	954.065346	15.719194
27.394887	955.390924	15.724211
27.667110	956.206397	15.729229
27.819551	965.805515	15.734247
27.667570	967.527032	15.739264
27.903085	966.393168	15.744282
27.580140	966.254398	15.749299
27.713271	967.139243	15.754317
28.024868	975.665392	15.759335
27.710986	972.819680	15.764352
27.628566	965.910270	15.769370
28.056530	968.377681	15.774387
28.068426	959.424111	15.779405
27.939144	968.398081	15.784423
27.716640	980.208821	15.789440
28.179975	971.955568	15.794458
28.036451	987.810389	15.799475
28.187649	976.020557	15.804493
27.951227	969.720849	15.809511
28.016036	973.685442	15.814528
28.183845	974.698459	15.819546
28.079399	980.338513	15.824563
28.131992	970.966328	15.829581
27.865611	978.213035	15.834599
28.046678	984.859868	15.839616
28.300998	978.507055	15.844634
27.916935	977.880976	15.849651
28.148160	970.998616	15.854669
28.352491	970.569693	15.859687
28.239986	978.620810	15.864704
28.132318	986.691609	15.869722
27.727663	981.746309	15.874739
28.194529	979.166171	15.879757
28.236356	997.130671	15.884775
28.482985	998.755586	15.889792
28.757616	995.926116	15.894810
28.866329	1008.088305	15.899827
28.725803	1009.600369	15.904845
28.357360	992.653850	15.909863
29.016051	997.078988	15.914880
28.943823	977.175258	15.919898
28.725129	974.635249	15.924915
28.740085	972.068987	15.929933
28.430339	966.628801	15.934951
28.305480	966.450574	15.939968
28.869078	976.544099	15.944986
28.872799	994.675116	15.950003
28.811854	995.647543	15.955021
28.636592	988.545297	15.960039
29.030199	986.731864	15.965056
29.249132	982.553812	15.970074
28.695311	988.032740	15.975091
28.945920	982.405655	15.980109
28.813451	975.383104	15.985127
29.065801	987.940776	15.990144
29.186417	990.642820	15.995162
29.228163	980.556660	16.000179
28.991345	974.856312	16.005197
29.010307	980.918686	16.010215
29.209463	982.208265	16.015232
28.791951	978.362945	16.020250
29.184303	980.900531	16.025267
28.875110	979.520072	16.030285
29.300745	987.972986	16.035303
28.857684	1002.016351	16.040320
29.358912	987.800225	16.045338
29.350291	990.335698	16.050355
29.042704	998.768711	16.055373
29.145782	996.196255	16.060391
29.166708	1004.182063	16.065408
29.406509	989.208563	16.070426
29.072463	1000.985202	16.075443
29.166869	999.302854	16.080461
29.316567	999.587332	16.085479
29.239126	1014.528761	16.090496
29.700017	1025.909658	16.095514
29.679223	1018.716698	16.100531
29.889152	1019.608174	16.105549
29.829553	1003.840872	16.110567
29.400984	995.923329	16.115584
29.661944	984.413276	16.120602
29.704969	1007.912860	16.125619
29.870579	1001.235998	16.130637
30.093933	987.912019	16.135655
29.625384	992.798498	16.140672
29.931699	989.737469	16.145690
29.910006	987.579728	16.150707
29.883271	990.612001	16.155725
29.881994	983.244492	16.160743
29.760268	985.667447	16.165760
29.725631	992.098583	16.170778
29.902285	1006.659718	16.175795
30.088907	1011.018584	16.180813
30.322442	1017.790765	16.185831
30.267430	1004.872949	16.190848
30.225516	984.358782	16.195866
30.244486	978.159905	16.200883
29.893838	978.341718	16.205901
30.142745	980.195921	16.210919
30.014276	984.260552	16.215936
30.210871	991.881722	16.220954
30.124133	996.411591	16.225971
30.237388	1005.367351	16.230989
30.527138	1001.682920	16.236007
30.091680	1017.673993	16.241024
30.556196	1005.195543	16.246042
30.738119	1010.550845	16.251059
30.507275	998.243075	16.256077
30.585938	972.644746	16.261095
30.091443	982.543675	16.266112
30.336621	970.451007	16.271130
30.688437	987.867427	16.276147
30.282605	990.817022	16.281165
30.627297	999.429139	16.286183
30.393243	1010.359311	16.291200
30.341371	997.582567	16.296218
30.595199	1003.006620	16.301235
30.439546	1004.160887	16.306253
30.542390	1008.069088	16.311271
30.458728	1005.488662	16.316288
30.714400	1004.442812	16.321306
30.636412	1009.188358	16.326323
30.474593	1004.987658	16.331341
30.660251	1010.807963	16.336359
30.490627	1015.983390	16.341376
30.888031	1028.022478	16.346394
31.019073	1033.302536	16.351411
31.209690	1030.385789	16.356429
30.969657	1036.900038	16.361447
31.247642	1040.020571	16.366464
31.272623	1017.365887	16.371482
31.094978	1010.194801	16.376499
30.892364	1006.559009	16.381517
30.962968	1015.219567	16.386535
30.938546	1034.346092	16.391552
31.184666	1030.626143	16.396570
31.300284	1028.654128	16.401587
31.134066	1034.793249	16.406605
31.298621	1027.267140	16.411623
30.969330	1040.406815	16.416640
31.156526	1034.099290	16.421658
31.212998	1040.898149	16.426675
31.131034	1040.643868	16.431693
31.540334	1043.236962	16.436711
31.210186	1036.849929	16.441728
31.395032	1036.553096	16.446746
31.484160	1042.870138	16.451763
31.563181	1041.227990	16.456781
31.510058	1038.921103	16.461799
31.272135	1038.561140	16.466816
31.319745	1036.741537	16.471834
31.450994	1044.157660	16.476851
31.529368	1060.644110	16.481869
32.128229	1054.079018	16.486887
31.983191	1068.545234	16.491904
32.064977	1046.790623	16.496922
31.865491	1031.064478	16.501939
32.070227	1030.029896	16.506957
32.081586	1015.766033	16.511975
32.060326	1023.975650	16.516992
31.905517	1022.625618	16.522010
32.199465	1016.261750	16.527027
31.989701	1024.682323	16.532045
32.082469	1025.483950	16.537063
31.950933	1026.843577	16.542080
31.589544	1023.693984	16.547098
31.859397	1008.515904	16.552115
32.004082	1022.523751	16.557133
32.195784	1022.864450	16.562151
31.893579	1032.932511	16.567168
31.932978	1023.954065	16.572186
32.227490	1033.884488	16.577203
32.199748	1051.916779	16.582221
32.536036	1036.523589	16.587239
32.311172	1054.346657	16.592256
32.451341	1042.125964	16.597274
32.381609	1030.685918	16.602291
32.200514	1036.089689	16.607309
32.614987	1036.973712	16.612327
32.458037	1037.640567	16.617344
32.442673	1056.517147	16.622362
32.708246	1053.950224	16.627379
32.428943	1062.388201	16.632397
32.711276	1050.352460	16.637415
32.496362	1051.874819	16.642432
32.510024	1043.919751	16.647450
33.021763	1055.446715	16.652467
32.634962	1060.172319	16.657485
32.718181	1047.271743	16.662503
32.585107	1048.510498	16.667520
32.887699	1049.874819	16.672538
33.148183	1037.870886	16.677555
32.660328	1042.595299	16.682573
32.771073	1045.558468	16.687591
32.841772	1044.277857	16.692608
32.756260	1045.722951	16.697626
33.126403	1051.304644	16.702643
32.946891	1051.858699	16.707661
32.757221	1046.981331	16.712679
32.817178	1052.176783	16.717696
32.538609	1058.277204	16.722714
32.752362	1048.482877	16.727731
32.729279	1047.206212	16.732749
33.189741	1066.606220	16.737767
33.301962	1062.434153	16.742784
33.513301	1061.198749	16.747802
33.317232	1054.990091	16.752819
33.281455	1048.447569	16.757837
33.532092	1045.241258	16.762855
33.117816	1043.822498	16.767872
33.170223	1050.658188	16.772890
33.843257	1062.785476	16.777907
33.208927	1061.603150	16.782925
33.414441	1063.067895	16.787943
33.472970	1066.753526	16.792960
33.209564	1069.477507	16.797978
33.724893	1063.318977	16.802995
33.388819	1068.352661	16.808013
33.936603	1063.242846	16.813031
33.856242	1070.356115	16.818048
33.372783	1070.865840	16.823066
33.869814	1061.809666	16.828083
33.788562	1066.598222	16.833101
33.859583	1067.280629	16.838119
34.068100	1061.746739	16.843136
33.879093	1059.535450	16.848154
34.051699	1064.316551	16.853171
33.872680	1067.796257	16.858189
33.889432	1060.059331	16.863207
33.820053	1064.007598	16.868224
33.904392	1075.133997	16.873242
34.083443	1065.249241	16.878259
33.836429	1073.757577	16.883277
33.793164	1069.986247	16.888295
33.855670	1061.521601	16.893312
33.971718	1072.375535	16.898330
34.176347	1064.158772	16.903347
33.986647	1070.347269	16.908365
34.168116	1067.823644	16.913383
34.294371	1057.088471	16.918400
34.172371	1062.369573	16.923418
34.132471	1060.848632	16.928435
33.968347	1072.384304	16.933453
34.454738	1084.352620	16.938471
34.630479	1083.159070	16.943488
34.476232	1088.300610	16.948506
34.726723	1082.868554	16.953523
34.243125	1093.382425	16.958541
34.549091	1092.091029	16.963559
34.774171	1088.412173	16.968576
34.454875	1086.394686	16.973594
35.137022	1085.950901	16.978611
34.747714	1088.341046	16.983629
34.822981	1098.514113	16.988647
35.073050	1087.597155	16.993664
34.758603	1086.805815	16.998682
34.831482	1085.897648	17.003699
34.771905	1086.018884	17.008717
34.819868	1081.215286	17.013735
35.119811	1090.275027	17.018752
34.937938	1090.727216	17.023770
35.152687	1084.328761	17.028787
34.886380	1081.643747	17.033805
34.796216	1093.809414	17.038823
34.830464	1091.413081	17.043840
34.751426	1090.395439	17.048858
34.875896	1083.589825	17.053875
34.791873	1086.451936	17.058893
35.046450	1082.178511	17.063911
34.966485	1087.465502	17.068928
34.909574	1089.670504	17.073946
35.044920	1092.110677	17.078963
35.122056	1110.477088	17.083981
35.208899	1116.585321	17.088999
35.531014	1114.103749	17.094016
35.577543	1118.821608	17.099034
35.593683	1104.663858	17.104051
35.383678	1120.790541	17.109069
35.608782	1110.953464	17.114087
35.674264	1117.579468	17.119104
35.644650	1120.072696	17.124122
35.470498	1112.499891	17.129139
35.929752	1126.394750	17.134157
36.098973	1106.910070	17.139175
36.046892	1111.594891	17.144192
35.647686	1097.130595	17.149210
35.842967	1093.281889	17.154227
35.928389	1107.668920	17.159245
36.021192	1098.623710	17.164263
35.961948	1081.088242	17.169280
35.614929	1083.097273	17.174298
36.172295	1078.184120	17.179315
36.281008	1086.679774	17.184333
35.961993	1084.231247	17.189351
35.967479	1081.315702	17.194368
35.971020	1081.346649	17.199386
36.205442	1094.140074	17.204403
36.055805	1095.969768	17.209421
35.912809	1102.437111	17.214439
36.424561	1094.366399	17.219456
36.177380	1106.796210	17.224474
36.465502	1100.699069	17.229491
36.345224	1097.243598	17.234509
36.194253	1105.994604	17.239527
36.346923	1091.986546	17.244544
36.442502	1099.559392	17.249562
36.496736	1097.504352	17.254579
36.561776	1099.900685	17.259597
36.277983	1094.306878	17.264615
36.594235	1094.586818	17.269632
36.019529	1103.490342	17.274650
36.481120	1099.149291	17.279667
36.510580	1104.006717	17.284685
36.329756	1101.641537	17.289703
36.437342	1103.271337	17.294720
36.440666	1124.455729	17.299738
37.012531	1133.102480	17.304755
36.924573	1129.673307	17.309773
36.965402	1124.655335	17.314791
37.175283	1121.963579	17.319808
36.980306	1134.915183	17.324826
37.122826	1128.938776	17.329843
37.066535	1110.603727	17.334861
36.722420	1104.533486	17.339879
37.396066	1112.088075	17.344896
37.126308	1114.624320	17.349914
36.909750	1110.053231	17.354931
36.745929	1114.998112	17.359949
36.913825	1129.370438	17.364967
36.887243	1127.270083	17.369984
36.885908	1135.913087	17.375002
37.215028	1137.523290	17.380019
37.322543	1127.012058	17.385037
37.169828	1129.828505	17.390055
37.396751	1135.613180	17.395072
37.186801	1127.153410	17.400090
37.319402	1120.281990	17.405107
37.629784	1142.934576	17.410125
37.612055	1151.919182	17.415143
38.049413	1132.854947	17.420160
37.405390	1132.852321	17.425178
37.560331	1127.657278	17.430195
37.723970	1126.431049	17.435213
37.594295	1137.211753	17.440231
38.124273	1134.608153	17.445248
37.771251	1133.454885	17.450266
37.855132	1126.904255	17.455283
37.803250	1127.612558	17.460301
37.696460	1146.592710	17.465319
38.038857	1146.462652	17.470336
38.209951	1149.867664	17.475354
37.979927	1148.546918	17.480371
38.007788	1152.152521	17.485389
38.036226	1148.759834	17.490407
38.372548	1145.587025	17.495424
37.861941	1154.129582	17.500442
38.502829	1146.403178	17.505459
38.392790	1148.254877	17.510477
38.253817	1151.073855	17.515495
38.514500	1137.559746	17.520512
38.147699	1140.131921	17.525530
37.987585	1141.908237	17.530547
38.211122	1145.476339	17.535565
37.908057	1150.701409	17.540583
38.171697	1142.506650	17.545600
38.104205	1147.266298	17.550618
38.291665	1134.448903	17.555635
38.348404	1146.974206	17.560653
38.312074	1163.317050	17.565671
38.550461	1160.310864	17.570688
38.723697	1180.069857	17.575706
38.588931	1176.512861	17.580723
38.890070	1172.751069	17.585741
38.512636	1166.933074	17.590759
38.654537	1166.797241	17.595776
38.885281	1177.821720	17.600794
39.013686	1172.409101	17.605811
39.178548	1171.783554	17.610829
39.014284	1170.046488	17.615847
38.996133	1174.769962	17.620864
38.660461	1171.823867	17.625882
38.881308	1172.120597	17.630899
38.806807	1169.124985	17.635917
38.850852	1181.285050	17.640935
39.300015	1171.289506	17.645952
39.146175	1181.931742	17.650970
39.124570	1167.389850	17.655987
39.006248	1175.665368	17.661005
39.113368	1187.804368	17.666023
39.494136	1192.015925	17.671040
39.476254	1193.882819	17.676058
39.605240	1205.966439	17.681075
39.804287	1201.319599	17.686093
39.648012	1182.577271	17.691111
39.286010	1161.948738	17.696128
39.046861	1179.351105	17.701146
39.403492	1187.060110	17.706163
39.827860	1187.686170	17.711181
39.553215	1203.744605	17.716199
40.174634	1190.003032	17.721216
39.922844	1194.707147	17.726234
39.895179	1197.920505	17.731251
40.074451	1179.138824	17.736269
39.996895	1189.345766	17.741287
40.212200	1182.116643	17.746304
40.028159	1179.718930	17.751322
39.942331	1158.360534	17.756339
39.755741	1156.148844	17.761357
39.537731	1172.144730	17.766375
39.983797	1175.420954	17.771392
39.922121	1184.842014	17.776410
39.913907	1186.759273	17.781427
39.871131	1182.243813	17.786445
39.866216	1185.288377	17.791463
40.233845	1193.484830	17.796480
40.054395	1192.704987	17.801498
40.255255	1207.363136	17.806515
40.633847	1216.102108	17.811533
40.260422	1217.676504	17.816551
40.631554	1202.194214	17.821568
40.736598	1207.681398	17.826586
40.574208	1205.550782	17.831603
40.746805	1199.333601	17.836621
40.887230	1211.237654	17.841639
41.042566	1193.199076	17.846656
41.072481	1177.769657	17.851674
40.663545	1171.898484	17.856691
40.910368	1167.140219	17.861709
40.663030	1171.220714	17.866727
40.595466	1174.863563	17.871744
40.751632	1172.716753	17.876762
40.852383	1196.957752	17.881779
41.150803	1196.098550	17.886797
41.076223	1201.795273	17.891815
41.126773	1171.025948	17.896832
40.984758	1173.549695	17.901850
40.658469	1182.103770	17.906867
41.098599	1190.703928	17.911885
41.114318	1196.782640	17.916903
40.908991	1209.484283	17.921920
41.032471	1201.738124	17.926938
41.149180	1205.475859	17.931955
41.141283	1202.011878	17.936973
41.112040	1199.042074	17.941991
41.253726	1205.360244	17.947008
41.066662	1206.315047	17.952026
41.156619	1222.411307	17.957043
41.334134	1219.768739	17.962061
41.426018	1231.721448	17.967079
41.766511	1218.565761	17.972096
41.832346	1220.987156	17.977114
41.624210	1219.566960	17.982131
41.920095	1215.200394	17.987149
41.828141	1220.272273	17.992167
41.826262	1221.166083	17.997184
41.450884	1222.020362	18.002202
41.525181	1214.069687	18.007219
41.680859	1217.563688	18.012237
41.630097	1231.272580	18.017255
41.609375	1222.740891	18.022272
41.864595	1235.888194	18.027290
41.853731	1247.945390	18.032307
42.414375	1254.030027	18.037325
42.576486	1255.128916	18.042343
42.431053	1248.128748	18.047360
42.226177	1236.868964	18.052378
42.408253	1254.267162	18.057395
42.584825	1245.705567	18.062413
42.476908	1228.412058	18.067431
42.357672	1223.369243	18.072448
42.982866	1224.754491	18.077466
42.490743	1221.189983	18.082483
42.194679	1221.918357	18.087501
42.168575	1233.790786	18.092519
42.456757	1239.873253	18.097536
42.512117	1252.041012	18.102554
42.599805	1260.551132	18.107571
43.037974	1246.407732	18.112589
42.888637	1258.796901	18.117607
42.775822	1261.174436	18.122624
42.824747	1258.591695	18.127642
43.086978	1254.994960	18.132659
43.187446	1244.144214	18.137677
42.984010	1250.300371	18.142695
43.317613	1246.365073	18.147712
43.348661	1236.569872	18.152730
42.771637	1229.339675	18.157747
43.161179	1234.973403	18.162765
42.986516	1252.659722	18.167783
42.995483	1245.694705	18.172800
43.195751	1253.906874	18.177818
43.221694	1250.621525	18.182835
43.305344	1251.775398	18.187853
43.028281	1254.337999	18.192871
43.295419	1245.757241	18.197888
43.432452	1250.553516	18.202906
42.914806	1261.157878	18.207923
43.304016	1247.695527	18.212941
43.256230	1243.419942	18.217959
43.234322	1259.960365	18.222976
43.175766	1265.876350	18.227994
43.589262	1273.194095	18.233011
44.039871	1272.057366	18.238029
43.720110	1280.509785	18.243047
43.595946	1275.580993	18.248064
43.947893	1269.580567	18.253082
43.499519	1283.024164	18.258099
43.970821	1270.133855	18.263117
44.112730	1274.894754	18.268135
43.895877	1270.753088	18.273152
44.225683	1263.999584	18.278170
44.403395	1270.864158	18.283187
44.252623	1264.599422	18.288205
43.976324	1264.775670	18.293223
44.379680	1269.084320	18.298240
44.308668	1255.898275	18.303258
43.893895	1260.081001	18.308275
44.405141	1255.272672	18.313293
44.566127	1267.879767	18.318311
44.477888	1261.194508	18.323328
44.580622	1253.034787	18.328346
44.085401	1260.280378	18.333363
44.218034	1254.596500	18.338381
44.291155	1269.254635	18.343399
44.876972	1287.439474	18.348416
45.020544	1272.531366	18.353434
44.839939	1280.842044	18.358451
45.145568	1276.423571	18.363469
44.721714	1266.184955	18.368487
44.849514	1258.024380	18.373504
45.029332	1244.548237	18.378522
45.090774	1256.077967	18.383539
45.259044	1258.876280	18.388557
45.033436	1255.745876	18.393575
44.842236	1258.058835	18.398592
45.134955	1245.024000	18.403610
44.532130	1262.176159	18.408627
44.932340	1278.603666	18.413645
45.112309	1279.600610	18.418663
44.776444	1291.624733	18.423680
45.169314	1283.649954	18.428698
45.340642	1294.064238	18.433715
45.356821	1285.971785	18.438733
45.186502	1283.597034	18.443751
45.327258	1293.781817	18.448768
45.482341	1288.383777	18.453786
45.150125	1297.327394	18.458803
45.565966	1302.326182	18.463821
45.708471	1300.060412	18.468839
45.701675	1312.079260	18.473856
45.772761	1302.872222	18.478874
45.943088	1314.804625	18.483891
46.067178	1314.717248	18.488909
46.094380	1300.949219	18.493927
46.132801	1287.331994	18.498944
46.199841	1274.455817	18.503962
46.127969	1282.171866	18.508979
46.053346	1285.479248	18.513997
46.172237	1277.343678	18.519015
45.976734	1273.923756	18.524032
46.385320	1272.766988	18.529050
45.847030	1280.332483	18.534067
46.432463	1277.058571	18.539085
46.298778	1279.201915	18.544103
45.860856	1273.122967	18.549120
46.289372	1291.996703	18.554138
46.029812	1303.555643	18.559155
46.467544	1299.890010	18.564173
46.358666	1297.524334	18.569191
46.385546	1309.968812	18.574208
46.367595	1309.488817	18.579226
46.468154	1310.753253	18.584243
46.381561	1302.796729	18.589261
46.658395	1313.835984	18.594279
46.359243	1311.878171	18.599296
46.713588	1320.630513	18.604314
46.802005	1339.067773	18.609331
46.683539	1335.302075	18.614349
47.044235	1329.533033	18.619367
46.926737	1329.199472	18.624384
47.424263	1331.721923	18.629402
47.290783	1340.902855	18.634419
47.215585	1330.382077	18.639437
47.601516	1336.606297	18.644455
47.023304	1336.048913	18.649472
47.372121	1326.229713	18.654490
47.353330	1336.820638	18.659507
47.257100	1338.564766	18.664525
47.492811	1324.936491	18.669543
47.070844	1333.878714	18.674560
47.393805	1326.482916	18.679578
47.473995	1329.208774	18.684595
47.161744	1337.295092	18.689613
47.473951	1341.294262	18.694631
47.490728	1338.422482	18.699648
47.596426	1328.225208	18.704666
47.715375	1334.704361	18.709683
47.581712	1344.162173	18.714701
48.111574	1347.922143	18.719719
48.065230	1356.157970	18.724736
48.095569	1332.737458	18.729754
47.875296	1328.866876	18.734771
48.032883	1320.904432	18.739789
48.082678	1326.807881	18.744807
47.877507	1345.381633	18.749824
48.148679	1346.629874	18.754842
48.445945	1352.443530	18.759859
48.383474	1354.489013	18.764877
48.139955	1339.285498	18.769895
48.280258	1342.811869	18.774912
48.467826	1343.327840	18.779930
48.300005	1351.861460	18.784947
48.405562	1345.555809	18.789965
48.346514	1344.863719	18.794983
48.367801	1365.784481	18.800000
48.522724	1347.159047	18.805018
48.589247	1339.967731	18.810035
48.599127	1351.221047	18.815053
48.503512	1341.007106	18.820071
48.434011	1347.577666	18.825088
48.511749	1344.219542	18.830106
48.590342	1359.167902	18.835123
48.825141	1366.525206	18.840141
49.085706	1370.370600	18.845159
49.186162	1376.695421	18.850176
49.156365	1369.661022	18.855194
49.518259	1374.338108	18.860211
49.086944	1375.382210	18.865229
49.273264	1366.763935	18.870247
49.145025	1369.227317	18.875264
49.542162	1362.157867	18.880282
49.408080	1371.022740	18.885299
49.514894	1365.264286	18.890317
49.684072	1369.144704	18.895335
49.562989	1374.240158	18.900352
49.378447	1378.705520	18.905370
49.665126	1369.937531	18.910387
49.487734	1364.795404	18.915405
49.441089	1366.136804	18.920423
49.780122	1366.251099	18.925440
49.979535	1361.072475	18.930458
49.649056	1362.467006	18.935475
49.383427	1364.834323	18.940493
50.102789	1360.799722	18.945511
49.812241	1354.370051	18.950528
49.853792	1359.288554	18.955546
49.933877	1363.401826	18.960563
50.074209	1365.661929	18.965581
50.105608	1356.560286	18.970599
50.104376	1362.599300	18.975616
50.214750	1373.498411	18.980634
50.410388	1377.715953	18.985651
50.385903	1384.685187	18.990669
50.459899	1384.547597	18.995687
49.872176	1398.381608	19.000704
50.283304	1383.592736	19.005722
50.457253	1386.371292	19.010739
50.379975	1376.547654	19.015757
50.216577	1384.501721	19.020775
50.220003	1382.258118	19.025792
50.470343	1379.548853	19.030810
50.583318	1392.632470	19.035827
50.540502	1418.800078	19.040845
50.965328	1402.860704	19.045863
50.868785	1413.649699	19.050880
50.598659	1420.378128	19.055898
51.036271	1407.117122	19.060915
51.010017	1413.090936	19.065933
51.349202	1420.330947	19.070951
51.011462	1410.669947	19.075968
51.458178	1403.218194	19.080986
51.503688	1413.166570	19.086003
51.265567	1416.726568	19.091021
51.469022	1405.428273	19.096039
51.272730	1416.667329	19.101056
51.132749	1414.866586	19.106074
51.403070	1408.838222	19.111091
51.326992	1413.122704	19.116109
51.210723	1402.345730	19.121127
51.312871	1412.234736	19.126144
51.487022	1411.033549	19.131162
51.860712	1428.475331	19.136179
51.640026	1444.821152	19.141197
51.621235	1428.460144	19.146215
51.678403	1440.346204	19.151232
51.831133	1442.200077	19.156250
51.851127	1429.553061	19.161267
51.820288	1436.347155	19.166285
52.135014	1438.996306	19.171303
51.855159	1437.184834	19.176320
51.821106	1440.273423	19.181338
52.196194	1438.445589	19.186355
52.326496	1459.581907	19.191373
52.748705	1450.067097	19.196391
52.249293	1447.689746	19.201408
52.440953	1443.239062	19.206426
52.931019	1452.194782	19.211443
52.414350	1434.310266	19.216461
52.384456	1428.645948	19.221479
52.616342	1444.104773	19.226496
52.685505	1450.066530	19.231514
52.872869	1438.649653	19.236531
52.709829	1459.533880	19.241549
52.948082	1450.644580	19.246567
53.220874	1456.803526	19.251584
53.079224	1450.178607	19.256602
53.205249	1443.492126	19.261619
53.173378	1433.474019	19.266637
53.127936	1415.839989	19.271655
52.885568	1422.156582	19.276672
52.946114	1431.374268	19.281690
53.471382	1448.252357	19.286707
53.314905	1457.965564	19.291725
53.609876	1445.224344	19.296743
53.395390	1432.570675	19.301760
52.804397	1420.710086	19.306778
53.202896	1443.447406	19.311795
53.226188	1447.856049	19.316813
53.178826	1449.057572	19.321831
53.555050	1449.189532	19.326848
53.657525	1454.910028	19.331866
53.373958	1446.465742	19.336883
52.980999	1451.856263	19.341901
53.439874	1463.970859	19.346919
53.560933	1473.386560	19.351936
54.001780	1472.391372	19.356954
53.864458	1477.583833	19.361971
53.801620	1471.605429	19.366989
54.336269	1473.049189	19.372007
54.106202	1469.301253	19.377024
54.126569	1468.340090	19.382042
54.364159	1477.611368	19.387059
54.229911	1463.442644	19.392077
54.485403	1467.641230	19.397095
54.798551	1460.440410	19.402112
54.261289	1465.169687	19.407130
54.802492	1464.037374	19.412147
54.929480	1463.246396	19.417165
54.840203	1455.672458	19.422183
54.946032	1462.438477	19.427200
54.982332	1464.290472	19.432218
55.212968	1464.497561	19.437235
54.914208	1469.265881	19.442253
54.925227	1464.093671	19.447271
55.166675	1456.493730	19.452288
54.782478	1464.527098	19.457306
55.111679	1456.280810	19.462323
54.874661	1463.062180	19.467341
54.898110	1464.782519	19.472359
54.795456	1467.675989	19.477376
54.900983	1455.296880	19.482394
54.854043	1468.108768	19.487411
54.665155	1482.824635	19.492429
55.196580	1496.510145	19.497447
55.406975	1488.182113	19.502464
55.341482	1487.450145	19.507482
55.333972	1485.848489	19.512499
55.028534	1494.610205	19.517517
55.316490	1494.952870	19.522535
55.525924	1513.808354	19.527552
55.781708	1517.568035	19.532570
56.376378	1502.817412	19.537587
56.154394	1513.769632	19.542605
55.814357	1502.668047	19.547623
56.205117	1493.040248	19.552640
55.957223	1493.018486	19.557658
56.013724	1491.216285	19.562675
55.990628	1509.555144	19.567693
56.088648	1518.353205	19.572711
56.190659	1510.077052	19.577728
55.966456	1515.815062	19.582746
56.372003	1518.086377	19.587763
56.153391	1519.028926	19.592781
56.279032	1511.703828	19.597799
56.167107	1507.815919	19.602816
56.018804	1513.714856	19.607834
56.463388	1514.421080	19.612851
56.784932	1527.584815	19.617869
56.732504	1535.234977	19.622887
56.723262	1526.455886	19.627904
56.607838	1541.345713	19.632922
57.252313	1534.447521	19.637939
57.161615	1541.274805	19.642957
56.910032	1540.715657	19.647975
57.108364	1538.417352	19.652992
56.986396	1539.942239	19.658010
56.933990	1537.757853	19.663027
56.775127	1546.180046	19.668045
57.020473	1541.256729	19.673063
57.205802	1542.732610	19.678080
57.069985	1539.513892	19.683098
57.197784	1528.921270	19.688115
57.286080	1543.877711	19.693133
57.264314	1552.850625	19.698151
57.621913	1549.367599	19.703168
57.687063	1558.963731	19.708186
57.702518	1555.646952	19.713203
57.443277	1556.886993	19.718221
57.798199	1557.459654	19.723239
57.953377	1558.067316	19.728256
57.735053	1559.793189	19.733274
58.237787	1552.036699	19.738291
57.994213	1563.841833	19.743309
58.061280	1559.506939	19.748327
58.094199	1546.881355	19.753344
57.928008	1565.178610	19.758362
57.917843	1554.123479	19.763379
58.033316	1567.109328	19.768397
58.291670	1581.683184	19.773415
58.573715	1577.516922	19.778432
58.374256	1586.187858	19.783450
58.829468	1586.730369	19.788467
58.880304	1588.611523	19.793485
59.176668	1571.327062	19.798503
58.987920	1558.867380	19.803520
58.499856	1558.861896	19.808538
58.601370	1547.666264	19.813555
58.649809	1558.081461	19.818573
58.500480	1572.882345	19.823591
58.626502	1582.135303	19.828608
58.517663	1587.044834	19.833626
59.210285	1580.720964	19.838643
59.210240	1584.961910	19.843661
59.011930	1582.088203	19.848679
59.231449	1580.772802	19.853696
58.976876	1585.961977	19.858714
58.785049	1584.293749	19.863731
59.373567	1599.711597	19.868749
59.426381	1605.948161	19.873767
59.852778	1601.148534	19.878784
59.369955	1610.349169	19.883802
59.453445	1606.862652	19.888819
59.513014	1604.089388	19.893837
59.570233	1609.777836	19.898855
59.754914	1599.989348	19.903872
59.758288	1602.724364	19.908890
59.869335	1605.266029	19.913907
59.447305	1605.666867	19.918925
59.890148	1613.930221	19.923943
60.340918	1619.985349	19.928960
59.960272	1640.992629	19.933978
60.573647	1624.882945	19.938995
60.445006	1635.288684	19.944013
60.476170	1640.024894	19.949031
60.881193	1621.058775	19.954048
60.242202	1616.937137	19.959066
60.737856	1601.544678	19.964083
60.238858	1615.646315	19.969101
60.455531	1617.420801	19.974119
60.939722	1620.623410	19.979136
60.607606	1626.905640	19.984154
60.659526	1625.920558	19.989171
60.696699	1626.452660	19.994189
60.859944	1625.868251	19.999207
60.755481	1620.467435	20.004224
60.523354	1621.047203	20.009242
61.121191	1619.908994	20.014259
60.903066	1621.324955	20.019277
60.597789	1632.273243	20.024295
61.045377	1640.704170	20.029312
60.868262	1651.045291	20.034330
61.316522	1646.205984	20.039347
61.535524	1646.905719	20.044365
61.014014	1644.877925	20.049383
61.102780	1656.677325	20.054400
61.094954	1673.931707	20.059418
61.387684	1680.537459	20.064435
61.937911	1682.930447	20.069453
61.505398	1689.403322	20.074471
62.041756	1676.055539	20.079488
61.933894	1686.830811	20.084506
62.167219	1676.856762	20.089523
62.228812	1673.469676	20.094541
62.211689	1671.729532	20.099559
62.545269	1667.904240	20.104576
62.373604	1674.886073	20.109594
62.173381	1668.776912	20.114611
62.232436	1666.785519	20.119629
62.372818	1668.989033	20.124647
62.456299	1667.969027	20.129664
62.007639	1673.175028	20.134682
62.261917	1655.956954	20.139699
62.630160	1668.223031	20.144717
62.404731	1667.225548	20.149735
62.506029	1666.163375	20.154752
62.923208	1685.147976	20.159770
63.094260	1686.215585	20.164787
63.073314	1692.718782	20.169805
62.951293	1704.117677	20.174823
63.298234	1687.402320	20.179840
63.044555	1693.675215	20.184858
63.040401	1693.114354	20.189875
63.304669	1687.717631	20.194893
63.214392	1697.577744	20.199911
63.378266	1686.243072	20.204928
63.330385	1689.450324	20.209946
63.488011	1687.583208	20.214963
63.455405	1689.699481	20.219981
63.356690	1695.191031	20.224999
63.449361	1688.822793	20.230016
63.249334	1693.443304	20.235034
63.580086	1692.681169	20.240051
63.782526	1692.749611	20.245069
63.677688	1708.743769	20.250087
64.083011	1717.516540	20.255104
64.020145	1716.474251	20.260122
64.085713	1722.991980	20.265139
64.260961	1718.930799	20.270157
64.141953	1719.637251	20.275175
64.654250	1710.905439	20.280192
64.571098	1725.895702	20.285210
64.287556	1719.826548	20.290227
64.693009	1716.154952	20.295245
64.330131	1729.824426	20.300263
64.654244	1712.172001	20.305280
64.367813	1726.408160	20.310298
64.664807	1725.339944	20.315315
64.567172	1716.941353	20.320333
64.186100	1726.324036	20.325351
64.380456	1719.039787	20.330368
64.670265	1722.731175	20.335386
64.436069	1739.913195	20.340403
65.066781	1741.675152	20.345421
65.077676	1748.942515	20.350439
64.830168	1739.734098	20.355456
64.903010	1748.709349	20.360474
64.857800	1749.094142	20.365491
65.400492	1754.349718	20.370509
65.226384	1771.152527	20.375527
65.564500	1761.691825	20.380544
65.878531	1778.921746	20.385562
65.431003	1781.170269	20.390579
65.517405	1759.797677	20.395597
65.608494	1766.857203	20.400615
65.925019	1766.831947	20.405632
65.641330	1768.332310	20.410650
65.818315	1762.866108	20.415667
66.106327	1768.061629	20.420685
65.788282	1770.157365	20.425703
66.166273	1755.415875	20.430720
66.272619	1767.539756	20.435738
65.817363	1759.440421	20.440755
66.193584	1758.408333	20.445773
66.211103	1786.270593	20.450791
66.527879	1789.542412	20.455808
66.583544	1793.914536	20.460826
66.761502	1793.102829	20.465843
66.733978	1794.869089	20.470861
66.675974	1795.034124	20.475879
67.157344	1778.042391	20.480896
67.196488	1781.715566	20.485914
67.022561	1767.611074	20.490931
67.092874	1766.942379	20.495949
67.273274	1756.305023	20.500967
67.246525	1747.096002	20.505984
66.963473	1742.727224	20.511002
66.819816	1763.622955	20.516019
67.391425	1767.959984	20.521037
67.373886	1765.625282	20.526055
67.502257	1775.010125	20.531072
67.698954	1772.762382	20.536090
67.495544	1770.246533	20.541107
67.577210	1774.430458	20.546125
67.329224	1773.290270	20.551143
67.830077	1768.439390	20.556160
67.861769	1765.027165	20.561178
67.611739	1780.460954	20.566195
67.924229	1775.528425	20.571213
67.733372	1774.821153	20.576231
67.617385	1772.170237	20.581248
67.945014	1782.283091	20.586266
67.883377	1798.978332	20.591283
68.282311	1805.200685	20.596301
68.311590	1807.893854	20.601319
68.402969	1794.912660	20.606336
68.556121	1801.057800	20.611354
68.178283	1803.071839	20.616371
68.684565	1796.126351	20.621389
68.366393	1806.982443	20.626407
68.351373	1797.154883	20.631424
68.505110	1810.990590	20.636442
68.530833	1823.973678	20.641459
68.800966	1819.508794	20.646477
68.831622	1827.468336	20.651495
68.922187	1830.423875	20.656512
69.050981	1829.366744	20.661530
69.192748	1831.935012	20.666547
69.456975	1819.267585	20.671565
69.298783	1825.424633	20.676583
69.202146	1831.436584	20.681600
69.582888	1822.345007	20.686618
69.212812	1834.648742	20.691635
68.969639	1813.957851	20.696653
69.299465	1841.576927	20.701671
69.472895	1852.532412	20.706688
69.747916	1850.467226	20.711706
69.489728	1859.877589	20.716723
69.444670	1851.453232	20.721741
69.583762	1866.650450	20.726759
69.858495	1858.895552	20.731776
70.294231	1874.305026	20.736794
70.443403	1880.358024	20.741811
70.862940	1874.978945	20.746829
70.665736	1852.024900	20.751847
70.464454	1845.050651	20.756864
70.802988	1832.525521	20.761882
70.569049	1849.301781	20.766899
70.710934	1839.439732	20.771917
70.507104	1843.678644	20.776935
70.462316	1840.970742	20.781952
70.641987	1852.274450	20.786970
70.776656	1860.698779	20.791987
71.064932	1874.086792	20.797005
70.942192	1880.437988	20.802023
70.735756	1871.471480	20.807040
70.977261	1868.730501	20.812058
70.510441	1880.577784	20.817075
71.123383	1873.775704	20.822093
71.478761	1865.138040	20.827111
71.217314	1868.454897	20.832128
71.743387	1870.749522	20.837146
71.601171	1879.652182	20.842163
71.557073	1861.194685	20.847181
71.583687	1869.153322	20.852199
71.892205	1884.957483	20.857216
72.285094	1881.976852	20.862234
72.137265	1888.357221	20.867251
72.032707	1879.412215	20.872269
72.008549	1868.725599	20.877287
71.966744	1884.775967	20.882304
72.212263	1888.210187	20.887322
71.953820	1895.548891	20.892339
71.913161	1889.035082	20.897357
72.129932	1884.564531	20.902375
71.977578	1883.096044	20.907392
72.036203	1894.014810	20.912410
72.218215	1910.351992	20.917427
72.746907	1905.008979	20.922445
73.069379	1902.126092	20.927463
72.640509	1910.374470	20.932480
72.945148	1900.203274	20.937498
73.059186	1906.806167	20.942515
73.166237	1901.940964	20.947533
72.983650	1894.817415	20.952551
72.657042	1902.509920	20.957568
73.016401	1901.326351	20.962586
72.790298	1900.096144	20.967603
73.050605	1897.054853	20.972621
73.288789	1895.676673	20.977639
72.865315	1916.579491	20.982656
73.513053	1923.238858	20.987674
73.219081	1931.717426	20.992691
73.429840	1930.233501	20.997709
73.668767	1932.630559	21.002727
73.727177	1926.722297	21.007744
74.007180	1918.346739	21.012762
73.491743	1937.675458	21.017779
73.907652	1948.836172	21.022797
74.154337	1952.959226	21.027815
74.391583	1956.681081	21.032832
74.245444	1958.046267	21.037850
74.233678	1957.989991	21.042867
74.360949	1950.672279	21.047885
74.547761	1953.615641	21.052903
74.379005	1945.137021	21.057920
74.776004	1948.194732	21.062938
74.468173	1950.712020	21.067955
74.666066	1958.921825	21.072973
74.625723	1943.350208	21.077991
74.652171	1951.560607	21.083008
75.093344	1971.010533	21.088026
75.051476	1981.029863	21.093043
75.195053	1980.863870	21.098061
75.012137	1981.586816	21.103079
75.241423	1981.442549	21.108096
75.599204	1972.857137	21.113114
75.554934	1981.613675	21.118131
75.977274	1973.238984	21.123149
75.937880	1972.156753	21.128167
75.699805	1971.905326	21.133184
75.716252	1971.987701	21.138202
75.497114	1974.902993	21.143219
75.339461	1971.656198	21.148237
75.537255	1971.440658	21.153255
75.545039	1984.648554	21.158272
75.857781	1983.040606	21.163290
75.823060	2003.060410	21.168307
75.986246	2000.143128	21.173325
76.244144	1988.508500	21.178343
76.078389	1999.986175	21.183360
76.274661	2000.853154	21.188378
76.251227	2006.222701	21.193395
76.420230	2021.449918	21.198413
76.632917	2025.629540	21.203431
76.689330	2022.748944	21.208448
77.235106	2023.406814	21.213466
76.844273	2027.917068	21.218483
76.771450	2023.571309	21.223501
77.315304	2023.465757	21.228519
76.784553	2035.344596	21.233536
77.102959	2012.905055	21.238554
76.919738	2026.337723	21.243571
77.348169	2013.642369	21.248589
77.317918	2013.409711	21.253607
77.099286	2015.554910	21.258624
77.467878	2021.229259	21.263642
77.489871	2034.965849	21.268659
77.465927	2048.458870	21.273677
77.908129	2049.209553	21.278695
77.993480	2053.949055	21.283712
78.007916	2048.502376	21.288730
77.691255	2042.329038	21.293747
77.562286	2037.278838	21.298765
78.086996	2042.903131	21.303783
77.909696	2042.462680	21.308800
78.253848	2055.764083	21.313818
78.299363	2066.945416	21.318835
78.551021	2068.446956	21.323853
78.586929	2068.453081	21.328871
78.595366	2073.321263	21.333888
78.989665	2063.333864	21.338906
78.762769	2068.192380	21.343923
78.778512	2061.989622	21.348941
78.749142	2072.677155	21.353959
78.588595	2072.583255	21.358976
78.947166	2066.490212	21.363994
78.851289	2065.214053	21.369011
78.641664	2086.791686	21.374029
79.137320	2093.556399	21.379047
79.157186	2098.263099	21.384064
79.335158	2096.229874	21.389082
79.273518	2095.768617	21.394099
79.557001	2095.618066	21.399117
79.379433	2091.903280	21.404135
79.362204	2107.477263	21.409152
79.752944	2115.139645	21.414170
79.954597	2125.017204	21.419187
80.139003	2110.787592	21.424205
80.175303	2112.650683	21.429223
80.189185	2121.521518	21.434240
80.363023	2117.178084	21.439258
80.338602	2113.013351	21.444275
79.809974	2113.078825	21.449293
80.325560	2111.711447	21.454311
80.182026	2115.245517	21.459328
80.487807	2131.552986	21.464346
80.482365	2135.392243	21.469363
80.648768	2137.413135	21.474381
81.149814	2137.248340	21.479399
80.930026	2143.584451	21.484416
81.259936	2144.167422	21.489434
81.268268	2143.067342	21.494451
81.313316	2129.224892	21.499469
81.242231	2127.144073	21.504487
81.154262	2142.065530	21.509504
81.127059	2128.638101	21.514522
81.182474	2137.074443	21.519539
81.038263	2136.731748	21.524557
81.433293	2135.452022	21.529575
81.315775	2160.835323	21.534592
81.481956	2155.841053	21.539610
81.981829	2159.908847	21.544627
81.788170	2164.640180	21.549645
82.097943	2162.651211	21.554663
81.891310	2179.686988	21.559680
82.107578	2156.398313	21.564698
82.202332	2156.697087	21.569715
82.033565	2156.797988	21.574733
82.070842	2169.434249	21.579751
82.589901	2176.297521	21.584768
82.339900	2183.067922	21.589786
82.712066	2193.153513	21.594803
82.538753	2175.633337	21.599821
82.878153	2169.194868	21.604839
82.779372	2188.243533	21.609856
82.704586	2185.641814	21.614874
83.002046	2181.479217	21.619891
82.658406	2185.531301	21.624909
83.083904	2203.040481	21.629927
83.159135	2214.539673	21.634944
83.417113	2210.156838	21.639962
83.486704	2211.821928	21.644979
83.327876	2214.016609	21.649997
83.434108	2209.178965	21.655015
83.362336	2208.135701	21.660032
83.482523	2215.241145	21.665050
83.749232	2230.716495	21.670067
83.845173	2232.894149	21.675085
83.902281	2247.345819	21.680103
84.087625	2235.378056	21.685120
84.376817	2231.495202	21.690138
84.382179	2242.248897	21.695155
84.591917	2241.111973	21.700173
84.619089	2227.398915	21.705191
84.330743	2239.570400	21.710208
84.496447	2226.726413	21.715226
84.693059	2228.323270	21.720243
84.654701	2240.373090	21.725261
84.690584	2247.771219	21.730279
84.915626	2263.885636	21.735296
85.068985	2258.719547	21.740314
85.077224	2266.339182	21.745331
85.052133	2261.962930	21.750349
85.647179	2251.745181	21.755367
85.140467	2261.461287	21.760384
85.368941	2267.475059	21.765402
85.597225	2260.299181	21.770419
85.290001	2258.181276	21.775437
85.410212	2268.929261	21.780455
85.460783	2262.650860	21.785472
85.232046	2270.280757	21.790490
85.429770	2270.194220	21.795507
85.914636	2276.193067	21.800525
86.211898	2277.243743	21.805543
85.940439	2278.528263	21.810560
85.731784	2275.336725	21.815578
86.120854	2276.981552	21.820595
86.119712	2298.814130	21.825613
86.005563	2297.030392	21.830631
86.525230	2300.544484	21.835648
86.479024	2293.849684	21.840666
86.890686	2294.353555	21.845683
86.640495	2307.526587	21.850701
86.936561	2288.334720	21.855719
86.722269	2299.808572	21.860736
86.851612	2308.976518	21.865754
87.095524	2317.338860	21.870771
86.922859	2329.462870	21.875789
87.518209	2323.698497	21.880807
87.523192	2317.870173	21.885824
87.383718	2314.015540	21.890842
87.545291	2322.142463	21.895859
87.438297	2321.769446	21.900877
87.899856	2317.752112	21.905895
87.826062	2327.121572	21.910912
87.788305	2334.582614	21.915930
88.254404	2345.745073	21.920947
88.102404	2347.388882	21.925965
88.385829	2357.159173	21.930983
88.212012	2352.644580	21.936000
88.161317	2350.297767	21.941018
88.387730	2348.415668	21.946035
88.068106	2357.722882	21.951053
88.476604	2354.450217	21.956071
88.548085	2352.028862	21.961088
88.422597	2368.646843	21.966106
88.752777	2373.750126	21.971123
88.821104	2368.757229	21.976141
88.984126	2377.141156	21.981159
88.626350	2371.951136	21.986176
88.756354	2376.443724	21.991194
89.058540	2395.778738	21.996211
89.195650	2411.562829	22.001229
89.368663	2399.909949	22.006247
89.312762	2401.774407	22.011264
89.453853	2407.850153	22.016282
89.528647	2408.989801	22.021299
89.640845	2419.629843	22.026317
89.777884	2425.719614	22.031335
89.870104	2423.738560	22.036352
90.159126	2437.288221	22.041370
90.270371	2429.765959	22.046387
90.296421	2433.683648	22.051405
90.392775	2429.115723	22.056423
90.693330	2430.095883	22.061440
90.479769	2435.550179	22.066458
90.646444	2424.924751	22.071475
90.536789	2428.579344	22.076493
90.778583	2431.583254	22.081511
90.920321	2417.075414	22.086528
90.799732	2422.589603	22.091546
90.880049	2426.391664	22.096563
90.639940	2452.463598	22.101581
91.440743	2450.375840	22.106599
91.735001	2447.419478	22.111616
91.016627	2471.434557	22.116634
91.468784	2463.299456	22.121651
91.626882	2448.513679	22.126669
91.647156	2450.153625	22.131687
91.715761	2452.092623	22.136704
91.546619	2455.194317	22.141722
91.790942	2451.917921	22.146739
91.758744	2460.758556	22.151757
92.055800	2460.918105	22.156775
92.051878	2464.905080	22.161792
91.920134	2467.713717	22.166810
92.296593	2471.337997	22.171827
92.132606	2475.204199	22.176845
92.436810	2480.465828	22.181863
92.312646	2486.494237	22.186880
92.499159	2492.380292	22.191898
92.944784	2502.728898	22.196915
92.850140	2508.146954	22.201933
93.225224	2500.378077	22.206951
93.349128	2493.285587	22.211968
93.199647	2500.908471	22.216986
93.496447	2501.458984	22.222003
93.711360	2491.279664	22.227021
93.739656	2497.922455	22.232039
93.863139	2498.822310	22.237056
93.708476	2497.138608	22.242074
93.569770	2490.884785	22.247091
93.644843	2494.055303	22.252109
93.748681	2489.181766	22.257127
93.931004	2500.194529	22.262144
93.540340	2521.529521	22.267162
93.902970	2514.251867	22.272179
94.102803	2519.568696	22.277197
93.948901	2526.534729	22.282215
94.239828	2523.731478	22.287232
94.343678	2538.448135	22.292250
94.648537	2537.823021	22.297267
94.752135	2552.922004	22.302285
94.525541	2549.927547	22.307303
94.707841	2541.369787	22.312320
94.785931	2546.097237	22.317338
94.991063	2545.837261	22.322355
95.014811	2545.892519	22.327373
95.171352	2557.980740	22.332391
95.101982	2565.544476	22.337408
95.067349	2568.268429	22.342426
95.510936	2563.336758	22.347443
95.125990	2567.422274	22.352461
95.425602	2573.523152	22.357479
95.918219	2572.737526	22.362496
96.077942	2600.839811	22.367514
96.375825	2591.182058	22.372531
96.255798	2603.191714	22.377549
96.459884	2597.168709	22.382567
96.525425	2587.821734	22.387584
96.745202	2591.113141	22.392602
96.956320	2585.465785	22.397619
97.013527	2587.522245	22.402637
96.540364	2578.202186	22.407655
96.975646	2580.958968	22.412672
96.955541	2588.632845	22.417690
97.087012	2590.914220	22.422707
96.900822	2597.776103	22.427725
96.825076	2591.713559	22.432743
97.114545	2586.227542	22.437760
96.857012	2604.368407	22.442778
97.170948	2593.674540	22.447795
97.459285	2609.514175	22.452813
97.560853	2620.339331	22.457831
97.594168	2615.702743	22.462848
97.443526	2625.076783	22.467866
97.619538	2622.375214	22.472883
97.778971	2614.156137	22.477901
98.020144	2642.632508	22.482919
98.291329	2642.793039	22.487936
98.173621	2658.640842	22.492954
98.575855	2644.072360	22.497971
98.616409	2640.724588	22.502989
98.517992	2646.950320	22.508007
98.680261	2644.239139	22.513024
98.865849	2647.866371	22.518042
98.446847	2642.261267	22.523059
99.083232	2643.032150	22.528077
99.289113	2656.354583	22.533095
99.207026	2651.318716	22.538112
99.133997	2655.842193	22.543130
99.316196	2654.800873	22.548147
99.214536	2658.586392	22.553165
99.143310	2661.604869	22.558183
99.717770	2648.359466	22.563200
99.602160	2652.446105	22.568218
99.429161	2667.502791	22.573235
99.491792	2676.049202	22.578253
99.752616	2683.336172	22.583271
99.994446	2686.311028	22.588288
99.698674	2686.398359	22.593306
100.033877	2683.935683	22.598323
100.038968	2695.101134	22.603341
99.849273	2695.011875	22.608359
100.121763	2694.428100	22.613376
100.373069	2710.008674	22.618394
100.516973	2727.774195	22.623411
100.637885	2737.482561	22.628429
100.930668	2736.792507	22.633447
101.265893	2725.721525	22.638464
101.134990	2735.820857	22.643482
101.492986	2731.918250	22.648499
101.263278	2739.752268	22.653517
101.466638	2744.644653	22.658535
101.938572	2745.817750	22.663552
101.729035	2743.923313	22.668570
102.109413	2741.651642	22.673587
102.043329	2744.231194	22.678605
101.769524	2757.598746	22.683623
102.092672	2755.024714	22.688640
102.061640	2758.419079	22.693658
101.990315	2754.232538	22.698675
102.193023	2741.731440	22.703693
102.255590	2755.278966	22.708711
102.688879	2761.083306	22.713728
102.639644	2771.223914	22.718746
102.953549	2769.176001	22.723763
102.946356	2785.474334	22.728781
102.868768	2780.971005	22.733799
103.121102	2775.394090	22.738816
102.997048	2781.240902	22.743834
103.059002	2778.559066	22.748851
103.391861	2774.758778	22.753869
103.352233	2780.146924	22.758887
103.300799	2786.264540	22.763904
103.438716	2802.076457	22.768922
103.585133	2797.655391	22.773939
103.766337	2800.581731	22.778957
103.632040	2804.789380	22.783975
104.060119	2818.494991	22.788992
104.387900	2819.941214	22.794010
104.598069	2825.554622	22.799027
104.691724	2831.219649	22.804045
104.724755	2824.564671	22.809063
104.781903	2827.941058	22.814080
104.928792	2833.838291	22.819098
104.721963	2827.833520	22.824115
104.822365	2822.051132	22.829133
104.809207	2830.228227	22.834151
105.005598	2819.950163	22.839168
105.062040	2828.073683	22.844186
105.191112	2845.034680	22.849203
105.411574	2852.212544	22.854221
105.241989	2847.379341	22.859239
105.368680	2844.660425	22.864256
105.421559	2849.604372	22.869274
105.582283	2845.570369	22.874291
105.757460	2849.053008	22.879309
105.741667	2869.800933	22.884327
106.415138	2880.619253	22.889344
106.152417	2879.630772	22.894362
106.507454	2879.006297	22.899379
106.525812	2876.200822	22.904397
106.264950	2878.522779	22.909415
106.408692	2878.160892	22.914432
106.748031	2879.261541	22.919450
106.516904	2870.847385	22.924467
106.468520	2891.952929	22.929485
106.406650	2900.398190	22.934503
106.895518	2898.001434	22.939520
106.888990	2908.389395	22.944538
107.376684	2923.707541	22.949555
107.552351	2932.579817	22.954573
107.743604	2937.445881	22.959591
108.028780	2920.116777	22.964608
107.764377	2932.702696	22.969626
107.913932	2923.535610	22.974643
108.280575	2923.718681	22.979661
107.845320	2934.113669	22.984679
108.060347	2926.247383	22.989696
108.396111	2953.608058	22.994714
108.275925	2949.909070	22.999731
108.359964	2954.215666	23.004749
108.502227	2951.194558	23.009767
108.667190	2944.420952	23.014784
108.709260	2951.036583	23.019802
108.764301	2955.155875	23.024819
109.137001	2964.550511	23.029837
109.113860	2975.597184	23.034855
109.267118	2969.400429	23.039872
109.338906	2986.141827	23.044890
109.203186	2977.788695	23.049907
109.441752	2968.577498	23.054925
109.463428	2985.256879	23.059943
109.880332	2990.186090	23.064960
109.969554	3003.801177	23.069978
109.912435	3007.497091	23.074995
110.255976	2997.344105	23.080013
110.140454	3006.185772	23.085031
110.294837	2998.286642	23.090048
110.556384	3002.059170	23.095066
110.169637	3025.967211	23.100083
110.785497	3021.154226	23.105101
110.847021	3019.130792	23.110119
110.847332	3026.509818	23.115136
111.082054	3035.384539	23.120154
110.928330	3019.988741	23.125171
111.043024	3017.071913	23.130189
111.199696	3027.768237	23.135207
111.660091	3032.994939	23.140224
111.622253	3034.442063	23.145242
111.702412	3050.759013	23.150259
111.951152	3043.298678	23.155277
111.744586	3056.488237	23.160295
111.929014	3043.516266	23.165312
111.959857	3052.436093	23.170330
111.935542	3049.326684	23.175347
112.135562	3038.468169	23.180365
111.865267	3053.841244	23.185383
112.323906	3066.635275	23.190400
112.689070	3077.658651	23.195418
112.377760	3075.504303	23.200435
112.616525	3066.001186	23.205453
112.722031	3086.813458	23.210471
113.059735	3087.964727	23.215488
113.698995	3100.422428	23.220506
113.243399	3091.358024	23.225523
113.723799	3095.702146	23.230541
113.410764	3102.286369	23.235559
113.442524	3097.560205	23.240576
113.686249	3101.381223	23.245594
113.428209	3103.082926	23.250611
113.851532	3101.983464	23.255629
113.712498	3129.285669	23.260647
114.055974	3136.404729	23.265664
114.480784	3128.152489	23.270682
114.418010	3128.157831	23.275699
114.749433	3116.770163	23.280717
114.857262	3126.711349	23.285735
114.727949	3122.124130	23.290752
114.816803	3115.465625	23.295770
114.835713	3136.337398	23.300787
115.380139	3133.156161	23.305805
115.425823	3152.684898	23.310823
115.380684	3148.031547	23.315840
115.110896	3147.918872	23.320858
115.143495	3150.501637	23.325875
115.603573	3140.296934	23.330893
115.496332	3154.970000	23.335911
115.487368	3170.273996	23.340928
115.787755	3169.145362	23.345946
115.936828	3170.527299	23.350963
116.084249	3170.735892	23.355981
116.112475	3189.749878	23.360999
116.686919	3187.672953	23.366016
116.605515	3192.614829	23.371034
116.573475	3199.982582	23.376051
116.970683	3191.890455	23.381069
116.755201	3205.093368	23.386087
116.545039	3188.175664	23.391104
116.860723	3203.094409	23.396122
117.002968	3219.727302	23.401139
117.221032	3217.086568	23.406157
117.121665	3238.214113	23.411175
116.928253	3230.236593	23.416192
117.591676	3234.304580	23.421210
117.651146	3250.105106	23.426227
118.087722	3248.557516	23.431245
117.850564	3238.218500	23.436263
117.922101	3257.799891	23.441280
118.504495	3246.140843	23.446298
118.435602	3239.479904	23.451315
118.728254	3236.597585	23.456333
118.513302	3235.511788	23.461351
118.859748	3257.761554	23.466368
118.780310	3269.529303	23.471386
118.691154	3275.183534	23.476403
119.217247	3266.710550	23.481421
119.352376	3265.937848	23.486439
119.367373	3266.999786	23.491456
119.459426	3272.657374	23.496474
119.493474	3279.176107	23.501491
119.663199	3262.756233	23.506509
119.715765	3284.116839	23.511527
119.818507	3289.514722	23.516544
120.019712	3286.685518	23.521562
119.853332	3301.481433	23.526579
120.145816	3290.278400	23.531597
120.095801	3293.010447	23.536615
120.206439	3302.380228	23.541632
120.688193	3299.808345	23.546650
120.505959	3316.559949	23.551667
120.522179	3315.770020	23.556685
120.836683	3314.106591	23.561703
120.984178	3327.694597	23.566720
121.164222	3336.092097	23.571738
121.437843	3343.669192	23.576755
121.921265	3348.383403	23.581773
121.742855	3342.178807	23.586791
122.143507	3344.825632	23.591808
122.360670	3328.855140	23.596826
122.124438	3337.938865	23.601843
122.035144	3330.315967	23.606861
122.111716	3333.691734	23.611879
122.081740	3331.801625	23.616896
122.341633	3325.859884	23.621914
121.986856	3345.402389	23.626931
122.411268	3348.824170	23.631949
122.351721	3367.223096	23.636967
122.328540	3375.875634	23.641984
122.680771	3385.699365	23.647002
122.920482	3395.629145	23.652019
123.214615	3401.550327	23.657037
122.847752	3401.403570	23.662055
123.519551	3422.244803	23.667072
123.821715	3427.032778	23.672090
123.410909	3429.723265	23.677107
123.679650	3425.089000	23.682125
123.920335	3426.190478	23.687143
124.120541	3426.109838	23.692160
124.413903	3420.945403	23.697178
124.101450	3424.158250	23.702195
124.552681	3411.470645	23.707213
124.079034	3433.373182	23.712231
124.288953	3430.835182	23.717248
124.828481	3427.780525	23.722266
124.479213	3437.741317	23.727283
125.000027	3445.882385	23.732301
125.154307	3459.003755	23.737319
125.101541	3468.353287	23.742336
125.188342	3458.685360	23.747354
125.000854	3465.001942	23.752371
125.433419	3476.923417	23.757389
125.692395	3484.638220	23.762407
125.788588	3496.289259	23.767424
125.762057	3494.080786	23.772442
125.713280	3493.708679	23.777459
126.116174	3496.655663	23.782477
126.364370	3512.125107	23.787495
126.453201	3517.769931	23.792512
126.624027	3519.308904	23.797530
126.677446	3524.672261	23.802547
126.626017	3516.059955	23.807565
126.888709	3518.149072	23.812583
127.057587	3537.348752	23.817600
127.970341	3526.561089	23.822618
127.660994	3532.410212	23.827635
127.673695	3528.371307	23.832653
128.032381	3528.437667	23.837671
127.876624	3527.122941	23.842688
127.958823	3515.849433	23.847706
128.225491	3522.951040	23.852723
128.292678	3524.615879	23.857741
128.272862	3524.492445	23.862759
128.431367	3518.960103	23.867776
128.679173	3539.931254	23.872794
128.514078	3552.763026	23.877811
128.602083	3557.209187	23.882829
129.119458	3548.522686	23.887847
128.944077	3562.227682	23.892864
128.907890	3552.585596	23.897882
128.912084	3562.662383	23.902899
129.077120	3579.107196	23.907917
129.358839	3578.116809	23.912935
129.376462	3587.461486	23.917952
129.320184	3592.322402	23.922970
129.728736	3603.874951	23.927987
129.849035	3615.781041	23.933005
130.293146	3604.104432	23.938023
130.077063	3615.734561	23.943040
130.258884	3631.266632	23.948058
130.469527	3643.582331	23.953075
130.425773	3642.951406	23.958093
130.654368	3635.421615	23.963111
130.865612	3638.247368	23.968128
131.251422	3635.231340	23.973146
130.829550	3646.072282	23.978163
130.892749	3655.007770	23.983181
131.521641	3656.342354	23.988199
131.245785	3659.241058	23.993216
131.475254	3658.970894	23.998234
131.594775	3672.057881	24.003251
132.046293	3676.136187	24.008269
132.061397	3684.394995	24.013287
132.062760	3698.762597	24.018304
132.488489	3679.398778	24.023322
132.500796	3675.957732	24.028339
132.382399	3690.353074	24.033357
132.697668	3694.930593	24.038375
132.762004	3715.629970	24.043392
132.722373	3697.719289	24.048410
133.025421	3722.038438	24.053427
133.098489	3708.669870	24.058445
133.343638	3710.388950	24.063463
133.525089	3732.617765	24.068480
133.595923	3723.859981	24.073498
133.633824	3740.481786	24.078515
133.647040	3741.793405	24.083533
134.063236	3739.333379	24.088551
134.270139	3751.196665	24.093568
134.748537	3750.111191	24.098586
134.702609	3758.902883	24.103603
134.896267	3760.187306	24.108621
135.177748	3753.447454	24.113639
134.740477	3758.179593	24.118656
135.149257	3748.573412	24.123674
135.251977	3750.345886	24.128691
134.940126	3753.832455	24.133709
135.217593	3758.078556	24.138727
135.040290	3774.684369	24.143744
135.387746	3781.990333	24.148762
135.554028	3791.656770	24.153779
135.553762	3796.234287	24.158797
136.108586	3815.433366	24.163815
136.077760	3830.761991	24.168832
135.851887	3822.887650	24.173850
136.171246	3820.053666	24.178867
136.205151	3829.248015	24.183885
136.292891	3839.008816	24.188903
136.368573	3847.423251	24.193920
136.560281	3860.248746	24.198938
136.960280	3868.859274	24.203955
137.275949	3876.524341	24.208973
137.250938	3869.557981	24.213991
137.350668	3872.186022	24.219008
137.778838	3879.796181	24.224026
138.254426	3892.795914	24.229043
138.084917	3897.588454	24.234061
138.403394	3896.099750	24.239079
138.561310	3889.025551	24.244096
138.403651	3888.121720	24.249114
138.710941	3879.065764	24.254131
138.328617	3891.244159	24.259149
138.774481	3884.310483	24.264167
138.573466	3885.349484	24.269184
139.013960	3885.327287	24.274202
139.221177	3874.658948	24.279219
138.940854	3892.884489	24.284237
138.967258	3902.411254	24.289255
139.026123	3904.435384	24.294272
139.100954	3917.821560	24.299290
139.384513	3933.690933	24.304307
139.343864	3940.610472	24.309325
140.050573	3947.919811	24.314343
139.854911	3964.137803	24.319360
140.057607	3967.677683	24.324378
140.434476	3975.797951	24.329395
140.283330	3977.281326	24.334413
140.675423	3977.047374	24.339431
141.011264	3993.392262	24.344448
141.113248	3988.931512	24.349466
141.326301	3993.945492	24.354483
141.055661	3996.265246	24.359501
141.761868	3978.606599	24.364519
141.395639	4015.422592	24.369536
141.276667	4019.644662	24.374554
141.804894	4012.980201	24.379571
141.860572	4028.417170	24.384589
142.085596	4034.910511	24.389607
142.477220	4045.201970	24.394624
142.443937	4043.411414	24.399642
142.655020	4051.413414	24.404659
142.688981	4043.362221	24.409677
143.187539	4036.298931	24.414695
143.298303	4047.959886	24.419712
143.463813	4042.875407	24.424730
143.331673	4032.718890	24.429747
143.129193	4061.712437	24.434765
143.678137	4066.576916	24.439783
143.597669	4065.173832	24.444800
143.710132	4055.871931	24.449818
143.588180	4075.639450	24.454835
143.992487	4081.434001	24.459853
144.562278	4092.722878	24.464871
144.568880	4094.250338	24.469888
144.819316	4105.156699	24.474906
144.930916	4092.259921	24.479923
144.677854	4096.133667	24.484941
144.996716	4111.249500	24.489959
145.325524	4105.167449	24.494976
145.713521	4103.806093	24.499994
146.251085	4096.507639	24.505011
145.847608	4106.376045	24.510029
146.210532	4097.644626	24.515047
145.974045	4108.276205	24.520064
146.206217	4110.080002	24.525082
146.416444	4099.772880	24.530099
146.475412	4102.872372	24.535117
146.490519	4096.417911	24.540135
146.620370	4107.361592	24.545152
146.298507	4103.909221	24.550170
146.645172	4103.877600	24.555187
146.305118	4114.501310	24.560205
146.898530	4121.891735	24.565223
146.997866	4122.676761	24.570240
147.152809	4133.608595	24.575258
147.365653	4142.632226	24.580275
147.445951	4158.776541	24.585293
147.834667	4145.302182	24.590311
147.717422	4160.385335	24.595328
148.060973	4183.467683	24.600346
148.165753	4185.812567	24.605363
148.279266	4192.089334	24.610381
148.242937	4183.877781	24.615399
148.811127	4196.396536	24.620416
148.751986	4217.843967	24.625434
149.029254	4205.272311	24.630451
148.934866	4218.823407	24.635469
149.135058	4212.692593	24.640487
149.539777	4226.471702	24.645504
149.481050	4219.093623	24.650522
149.617160	4237.722828	24.655539
149.592695	4233.602335	24.660557
150.001649	4229.931934	24.665575
150.465930	4254.002852	24.670592
150.350933	4246.060257	24.675610
150.644283	4253.264168	24.680627
151.026748	4252.953083	24.685645
151.102520	4252.664151	24.690663
151.018630	4253.985005	24.695680
151.076634	4249.966998	24.700698
151.272678	4251.352565	24.705715
151.368047	4274.089949	24.710733
151.211391	4274.094526	24.715751
151.541550	4270.892940	24.720768
151.231665	4282.376499	24.725786
151.774865	4287.415035	24.730803
151.832587	4304.666795	24.735821
152.157044	4301.525112	24.740839
152.320043	4321.104356	24.745856
152.419874	4322.369964	24.750874
152.829843	4322.080453	24.755891
152.690050	4328.407892	24.760909
153.245848	4324.176766	24.765927
153.327348	4342.183908	24.770944
153.852228	4354.150387	24.775962
153.788014	4353.856239	24.780979
153.817307	4354.108073	24.785997
153.917102	4362.786426	24.791015
153.923264	4347.816854	24.796032
154.023791	4352.935433	24.801050
154.641485	4333.398551	24.806067
154.051584	4343.694889	24.811085
154.335942	4349.823339	24.816103
154.783103	4354.493320	24.821120
154.908680	4373.152697	24.826138
155.124520	4359.265174	24.831155
154.973420	4371.687150	24.836173
154.985382	4365.093832	24.841191
155.192795	4381.140245	24.846208
155.192233	4397.201742	24.851226
155.534399	4386.857651	24.856243
155.542337	4404.752305	24.861261
155.926086	4408.647320	24.866279
156.113721	4414.202792	24.871296
155.891428	4430.275291	24.876314
156.378915	4427.801429	24.881331
156.701424	4453.375789	24.886349
157.020958	4444.223923	24.891367
157.609655	4446.573509	24.896384
157.673042	4440.533640	24.901402
157.808810	4442.531424	24.906419
157.488680	4435.183900	24.911437
158.002745	4437.815211	24.916455
158.259877	4430.033453	24.921472
158.039527	4437.025930	24.926490
158.195523	4427.992187	24.931507
158.296969	4436.627841	24.936525
158.511467	4444.399807	24.941543
158.394254	4465.550844	24.946560
158.465083	4464.175519	24.951578
158.670766	4464.460592	24.956595
159.033591	4482.906856	24.961613
159.226873	4481.139124	24.966631
159.291594	4482.887853	24.971648
159.331656	4487.667624	24.976666
159.289700	4490.429288	24.981683
159.521626	4511.033056	24.986701
159.651545	4509.634145	24.991719
159.842129	4509.503118	24.996736
160.184667	4524.361510	25.001754
160.630812	4525.697790	25.006771
160.911310	4541.374791	25.011789
160.701479	4539.779883	25.016807
161.030439	4535.978201	25.021824
161.064866	4554.202364	25.026842
161.384049	4562.764830	25.031859
161.117955	4572.847644	25.036877
161.151206	4568.329238	25.041895
161.475200	4570.829610	25.046912
161.432477	4598.046817	25.051930
162.146979	4592.507244	25.056947
161.886972	4609.304972	25.061965
161.825684	4597.214913	25.066983
162.257864	4608.684256	25.072000
162.382432	4630.110080	25.077018
162.489122	4623.448836	25.082035
162.579790	4631.253230	25.087053
162.799460	4643.462133	25.092071
163.281635	4646.623283	25.097088
163.284734	4655.911956	25.102106
163.520036	4654.246066	25.107123
163.781077	4673.663828	25.112141
164.178282	4675.601083	25.117159
164.134378	4681.310787	25.122176
164.185545	4676.625075	25.127194
164.221615	4676.420346	25.132211
164.206020	4685.832381	25.137229
164.706981	4703.453698	25.142247
164.835855	4697.515778	25.147264
164.956817	4698.659261	25.152282
165.067675	4713.887551	25.157299
165.304650	4720.727794	25.162317
164.970999	4722.803605	25.167335
165.304772	4730.119310	25.172352
165.477782	4740.687630	25.177370
165.541708	4757.133367	25.182387
165.967113	4766.624614	25.187405
166.186552	4780.418053	25.192423
166.541009	4780.924075	25.197440
166.281736	4796.595364	25.202458
166.651625	4793.337773	25.207475
167.221076	4807.748839	25.212493
167.202553	4811.785982	25.217511
167.417463	4807.922172	25.222528
167.491858	4806.055353	25.227546
167.545984	4825.089360	25.232563
167.804948	4824.370786	25.237581
167.689512	4845.269558	25.242599
168.357742	4846.129915	25.247616
168.519661	4869.831535	25.252634
168.899615	4856.237564	25.257651
168.866832	4875.751213	25.262669
168.417096	4872.221493	25.267687
168.910681	4871.615769	25.272704
169.300817	4895.322740	25.277722
169.468724	4898.917957	25.282739
169.899527	4890.441153	25.287757
169.744157	4899.497997	25.292775
169.912074	4889.589629	25.297792
169.798945	4913.123550	25.302810
170.107895	4922.508381	25.307827
170.433089	4923.223615	25.312845
170.412563	4929.068933	25.317863
170.927944	4927.332399	25.322880
170.649719	4947.182644	25.327898
170.833632	4962.088799	25.332915
171.396692	4953.103909	25.337933
171.007437	4952.341563	25.342951
171.764034	4946.865953	25.347968
171.568619	4956.509797	25.352986
171.820033	4959.884028	25.358003
172.116557	4974.615690	25.363021
171.974974	4976.267564	25.368039
172.303916	4974.990286	25.373056
172.552692	4981.137263	25.378074
172.397931	5000.303923	25.383091
172.682060	4992.125004	25.388109
172.860859	5002.522663	25.393127
173.160482	5007.656931	25.398144
172.984495	5019.743566	25.403162
173.736894	5026.777124	25.408179
174.019446	5023.444511	25.413197
173.907257	5024.702288	25.418215
173.996471	5031.044652	25.423232
174.214059	5031.723552	25.428250
174.410277	5039.029875	25.433267
174.642464	5042.114539	25.438285
174.579885	5045.458606	25.443303
175.111336	5043.923253	25.448320
174.843038	5073.244752	25.453338
174.844544	5069.007386	25.458355
175.627831	5072.175696	25.463373
175.461975	5095.884308	25.468391
175.564168	5102.183726	25.473408
175.619474	5096.137009	25.478426
176.059635	5113.978566	25.483443
176.410175	5118.007303	25.488461
176.599748	5134.160444	25.493479
176.830808	5113.207532	25.498496
176.772413	5135.961325	25.503514
176.986382	5137.226116	25.508531
177.712069	5133.263483	25.513549
177.628545	5149.946365	25.518567
177.980195	5142.489022	25.523584
177.721824	5135.914069	25.528602
177.993280	5133.465098	25.533619
177.789893	5158.852331	25.538637
177.861296	5167.659987	25.543655
178.189227	5160.579316	25.548672
178.748957	5186.117923	25.553690
178.856404	5200.402424	25.558707
179.483669	5192.291416	25.563725
179.152562	5195.362858	25.568743
179.447748	5191.300488	25.573760
179.658866	5196.891064	25.578778
179.663821	5207.048315	25.583795
180.042603	5214.899133	25.588813
180.150217	5220.348090	25.593831
180.301153	5215.341844	25.598848
180.310007	5207.328633	25.603866
180.343908	5226.358516	25.608883
180.591891	5228.826280	25.613901
180.957429	5230.996021	25.618919
180.984442	5246.973805	25.623936
181.103238	5233.029342	25.628954
181.496540	5254.450209	25.633971
181.804256	5259.617105	25.638989
181.880845	5261.796728	25.644007
182.097726	5259.887468	25.649024
182.188397	5259.124902	25.654042
182.188796	5271.281174	25.659059
182.082160	5266.566149	25.664077
182.363581	5282.143884	25.669095
182.799564	5283.052315	25.674112
182.829586	5303.055294	25.679130
183.135891	5309.138955	25.684148
183.285790	5326.556591	25.689165
183.057144	5331.339352	25.694183
183.717914	5347.301174	25.699200
183.841669	5345.466541	25.704218
183.896340	5358.784080	25.709236
183.991046	5371.531173	25.714253
184.236592	5378.928929	25.719271
184.614070	5387.550245	25.724288
184.507874	5391.976789	25.729306
184.948034	5409.867483	25.734324
185.209130	5403.516414	25.739341
185.388330	5419.464616	25.744359
185.964163	5423.107431	25.749376
186.258897	5432.017318	25.754394
186.193819	5444.044134	25.759412
186.424844	5431.753376	25.764429
186.076840	5435.871539	25.769447
186.353404	5434.294966	25.774464
186.723406	5459.158607	25.779482
186.662514	5459.938569	25.784500
187.099691	5452.926883	25.789517
186.791427	5465.506216	25.794535
187.700167	5481.057319	25.799552
187.748382	5482.082653	25.804570
187.479862	5489.629291	25.809588
188.281488	5487.203523	25.814605
188.232544	5502.991506	25.819623
188.548477	5500.637660	25.824640
188.765883	5499.175933	25.829658
189.064221	5487.919169	25.834676
189.189351	5510.990441	25.839693
188.967403	5531.361964	25.844711
189.216240	5527.656200	25.849728
189.546129	5538.499828	25.854746
189.356152	5545.995423	25.859764
189.746453	5551.154765	25.864781
189.505810	5561.834466	25.869799
190.085814	5567.768393	25.874816
190.209223	5582.411042	25.879834
190.455074	5593.043890	25.884852
190.626084	5589.526746	25.889869
190.557229	5608.499551	25.894887
190.853584	5611.290883	25.899904
191.120182	5616.244964	25.904922
191.241233	5641.820471	25.909940
191.823310	5642.173018	25.914957
192.059542	5653.893922	25.919975
191.993661	5647.512270	25.924992
192.265091	5652.506503	25.930010
192.242711	5677.101065	25.935028
192.655316	5673.008832	25.940045
192.256606	5676.663890	25.945063
192.808994	5697.477858	25.950080
193.408919	5691.648541	25.955098
193.302390	5694.117044	25.960116
193.655085	5694.951454	25.965133
193.824773	5706.933977	25.970151
194.197731	5718.767668	25.975168
194.081997	5724.143849	25.980186
194.275540	5720.832353	25.985204
194.859761	5731.449122	25.990221
194.852678	5743.903576	25.995239
195.068823	5741.915700	26.000256
195.316506	5741.201245	26.005274
195.220221	5751.448965	26.010292
195.522899	5763.072822	26.015309
196.025048	5769.271002	26.020327
196.307616	5764.762048	26.025344
196.647935	5763.510430	26.030362
196.502748	5761.997913	26.035380
196.624978	5780.888552	26.040397
196.447793	5783.705845	26.045415
197.013817	5788.793201	26.050432
197.298020	5791.621122	26.055450
196.863050	5809.721838	26.060468
197.463209	5823.189645	26.065485
197.743978	5825.090552	26.070503
197.982818	5840.235879	26.075520
197.798339	5852.874480	26.080538
198.147744	5862.391147	26.085556
198.394226	5856.146854	26.090573
198.816462	5869.380296	26.095591
198.933563	5878.876575	26.100608
199.294079	5869.110720	26.105626
199.048258	5881.475897	26.110644
199.165097	5895.049143	26.115661
199.600228	5897.332986	26.120679
199.837225	5900.557107	26.125696
200.170180	5921.515733	26.130714
200.376660	5929.280327	26.135732
200.454709	5915.772854	26.140749
200.704305	5928.120458	26.145767
201.033494	5957.241461	26.150784
201.495583	5944.445327	26.155802
201.199883	5953.883943	26.160820
201.342113	5954.744054	26.165837
201.743035	5951.226363	26.170855
201.496782	5956.880702	26.175872
201.910282	5966.193679	26.180890
201.988851	5994.827587	26.185908
202.301238	5979.499920	26.190925
202.805262	6001.295241	26.195943
202.639952	6009.411031	26.200960
202.945597	6016.565077	26.205978
202.710760	6025.769811	26.210996
202.966283	6027.917876	26.216013
203.145734	6036.166754	26.221031
203.712412	6046.439592	26.226048
203.749457	6054.586875	26.231066
203.911944	6064.009951	26.236084
204.143771	6076.306225	26.241101
204.655890	6084.621685	26.246119
204.406502	6095.018357	26.251136
204.954998	6109.544198	26.256154
205.101163	6113.036183	26.261172
205.544207	6105.813980	26.266189
205.764354	6132.132187	26.271207
205.635833	6148.282865	26.276224
206.206309	6139.325983	26.281242
206.196290	6140.284331	26.286260
206.731464	6163.969445	26.291277
206.806543	6163.552346	26.296295
206.806846	6179.534611	26.301312
207.341329	6177.285865	26.306330
207.044281	6183.839788	26.311348
207.579661	6196.179036	26.316365
207.482182	6200.862489	26.321383
207.856282	6207.347196	26.326400
208.256467	6218.467290	26.331418
207.865981	6237.801373	26.336436
208.360754	6233.169546	26.341453
208.721347	6252.764710	26.346471
208.798601	6253.960918	26.351488
209.528629	6265.769600	26.356506
209.436445	6275.921043	26.361524
209.885314	6280.747948	26.366541
210.193194	6277.183647	26.371559
210.001759	6275.804331	26.376576
210.924067	6271.047691	26.381594
210.914093	6279.297005	26.386612
211.343634	6279.070443	26.391629
211.493965	6276.261377	26.396647
211.397881	6289.867356	26.401664
211.777498	6280.649712	26.406682
211.598642	6288.420063	26.411700
211.637310	6283.073377	26.416717
211.440700	6291.985011	26.421735
211.799679	6304.225802	26.426752
212.167998	6308.449518	26.431770
211.712827	6327.644543	26.436788
211.724123	6329.425614	26.441805
212.643051	6358.019887	26.446823
212.624187	6369.925220	26.451840
213.195995	6372.491047	26.456858
213.190895	6391.754453	26.461876
213.682857	6391.412512	26.466893
213.729950	6402.740094	26.471911
213.819121	6404.284529	26.476928
214.082407	6424.141693	26.481946
214.239681	6427.989964	26.486964
214.868529	6441.046220	26.491981
215.327395	6454.061135	26.496999
215.316087	6461.877250	26.502016
215.749204	6452.575441	26.507034
215.409270	6461.521826	26.512052
215.613621	6481.135120	26.517069
215.949935	6482.348272	26.522087
215.834756	6485.627877	26.527104
216.191743	6504.585088	26.532122
216.425549	6518.824760	26.537140
216.595616	6530.281538	26.542157
217.164473	6536.116936	26.547175
217.137962	6546.114900	26.552192
217.405203	6562.445269	26.557210
217.426396	6565.176796	26.562228
217.904014	6578.007085	26.567245
218.261321	6598.943124	26.572263
218.201078	6612.210089	26.577280
218.728308	6596.487979	26.582298
218.581925	6626.189655	26.587316
219.050624	6630.458833	26.592333
219.461979	6629.615181	26.597351
219.597520	6644.323040	26.602368
219.922117	6651.037709	26.607386
220.044490	6655.030865	26.612404
220.337009	6653.922912	26.617421
220.468950	6663.045181	26.622439
220.859295	6670.734436	26.627456
220.874181	6669.531478	26.632474
221.180533	6683.041407	26.637492
221.434060	6702.988622	26.642509
221.809104	6692.158537	26.647527
221.636435	6705.253891	26.652544
222.024287	6708.139429	26.657562
222.043122	6724.259376	26.662580
222.646497	6725.673882	26.667597
222.443483	6725.864442	26.672615
222.433825	6754.487133	26.677632
222.672913	6755.834613	26.682650
222.876192	6769.730845	26.687668
223.056404	6785.456915	26.692685
223.684205	6800.164351	26.697703
223.638347	6808.807570	26.702720
224.355818	6815.236238	26.707738
224.452524	6813.962003	26.712756
224.665875	6827.322449	26.717773
224.951556	6834.137035	26.722791
224.941437	6851.192515	26.727808
225.162667	6835.442614	26.732826
225.322961	6859.271219	26.737844
225.295416	6868.379698	26.742861
225.531156	6872.355628	26.747879
225.879780	6894.212450	26.752896
225.767463	6902.956013	26.757914
225.838798	6924.176499	26.762932
226.770559	6929.803142	26.767949
226.869748	6933.357887	26.772967
226.990019	6956.492775	26.777984
227.616927	6956.635229	26.783002
227.645548	6961.610393	26.788020
227.645794	6971.547729	26.793037
228.387170	6967.553022	26.798055
228.255398	6986.142645	26.803072
228.661686	6991.794066	26.808090
228.866828	7002.882115	26.813108
229.096655	7014.599617	26.818125
229.121693	7015.188929	26.823143
229.272467	7032.595063	26.828160
229.489247	7043.226514	26.833178
229.808938	7053.732987	26.838196
229.821963	7071.298030	26.843213
229.932977	7074.112897	26.848231
230.435403	7091.138093	26.853248
230.641487	7097.122816	26.858266
231.105127	7118.939606	26.863284
231.398680	7127.344005	26.868301
231.927185	7133.079071	26.873319
231.961248	7142.078759	26.878336
232.207895	7154.082449	26.883354
232.532562	7159.513262	26.888372
232.865183	7156.575049	26.893389
233.158199	7155.986279	26.898407
233.091373	7169.403499	26.903424
233.112088	7178.997807	26.908442
233.532793	7181.232230	26.913460
233.514497	7186.139414	26.918477
233.897875	7192.177743	26.923495
233.743925	7223.506592	26.928512
234.354133	7224.466070	26.933530
234.311498	7229.447961	26.938548
234.445160	7247.027028	26.943565
234.465603	7269.302588	26.948583
234.812127	7280.883676	26.953600
235.454239	7299.760264	26.958618
235.289338	7312.101925	26.963636
235.912487	7316.775505	26.968653
236.402105	7334.838481	26.973671
236.317279	7338.721649	26.978688
236.479877	7355.401614	26.983706
236.746267	7370.629097	26.988724
236.533908	7370.223166	26.993741
237.078076	7393.971768	26.998759
237.246999	7399.842941	27.003776
237.705835	7410.572192	27.008794
237.915514	7422.169696	27.013812
237.991049	7429.677417	27.018829
238.301058	7436.485258	27.023847
238.175225	7462.011205	27.028864
238.610977	7461.100677	27.033882
239.494443	7473.791520	27.038900
239.585785	7474.527648	27.043917
239.688133	7485.578941	27.048935
239.963062	7503.829778	27.053952
240.082462	7500.086724	27.058970
240.325016	7510.955173	27.063988
240.343255	7532.891568	27.069005
240.800433	7528.974280	27.074023
240.913023	7547.819928	27.079040
241.383652	7564.011973	27.084058
241.511814	7567.852595	27.089076
241.712112	7587.539602	27.094093
242.065896	7590.604640	27.099111
242.358583	7605.268733	27.104128
242.456874	7620.015758	27.109146
242.758500	7616.230253	27.114164
242.815350	7629.968874	27.119181
243.446010	7641.719760	27.124199
243.559595	7657.835059	27.129216
243.599694	7656.466700	27.134234
244.021657	7665.435560	27.139252
243.853742	7678.645889	27.144269
244.072545	7699.746409	27.149287
244.612309	7700.771444	27.154304
244.700481	7727.173716	27.159322
244.992387	7740.576758	27.164340
245.085053	7756.489344	27.169357
245.813262	7759.099739	27.174375
245.853558	7770.929882	27.179392
246.295105	7791.951751	27.184410
246.745981	7790.253522	27.189428
246.858802	7809.984669	27.194445
246.985580	7819.612055	27.199463
247.048869	7822.370152	27.204480
247.343047	7836.019988	27.209498
247.617126	7856.810557	27.214516
247.860638	7853.980837	27.219533
248.205396	7869.521311	27.224551
248.042930	7887.965089	27.229568
248.849613	7895.623245	27.234586
248.792062	7914.608211	27.239604
248.784152	7922.182988	27.244621
248.960788	7929.887298	27.249639
249.563950	7945.312698	27.254656
249.685354	7975.356005	27.259674
250.091640	7977.433907	27.264692
250.014264	7987.192300	27.269709
250.490494	7988.815268	27.274727
250.930200	8005.290486	27.279744
251.255613	8004.755538	27.284762
251.527550	8014.082152	27.289780
251.610481	8025.119630	27.294797
251.880992	8030.472844	27.299815
252.117650	8039.266886	27.304832
251.908555	8059.642967	27.309850
252.508325	8056.915369	27.314868
252.540930	8084.084484	27.319885
252.986492	8089.242216	27.324903
252.819137	8100.361348	27.329920
252.866066	8120.551920	27.334938
253.129104	8124.962123	27.339956
253.356962	8158.134714	27.344973
253.702540	8161.412847	27.349991
254.092530	8190.653664	27.355008
254.375917	8209.635021	27.360026
255.000499	8220.868006	27.365044
255.091383	8241.946407	27.370061
255.661671	8252.010125	27.375079
255.910508	8265.673879	27.380096
256.236181	8267.218584	27.385114
256.365347	8275.697053	27.390132
256.325448	8298.608547	27.395149
256.757138	8305.173135	27.400167
257.117583	8327.658899	27.405184
257.155958	8341.178435	27.410202
257.670478	8348.633173	27.415220
257.792849	8366.181526	27.420237
258.341793	8370.564329	27.425255
258.598793	8387.820563	27.430272
258.686636	8398.786716	27.435290
259.014627	8387.013147	27.440308
259.120056	8413.054674	27.445325
259.373685	8426.831909	27.450343
259.682106	8444.712665	27.455360
259.873960	8453.924059	27.460378
260.163331	8462.632048	27.465396
260.250440	8479.620387	27.470413
260.857140	8488.540631	27.475431
261.267243	8510.656791	27.480448
261.454382	8512.292062	27.485466
261.705611	8518.668330	27.490484
261.695172	8543.571044	27.495501
261.969580	8546.733134	27.500519
262.216283	8556.287980	27.505536
262.523352	8579.910243	27.510554
262.725330	8590.968116	27.515572
262.536734	8603.574685	27.520589
262.891422	8624.992827	27.525607
263.327822	8645.314032	27.530624
263.342124	8653.591481	27.535642
263.930153	8668.735587	27.540660
264.001322	8673.065978	27.545677
264.503449	8695.658373	27.550695
264.954382	8705.013548	27.555712
264.670200	8706.599636	27.560730
265.386974	8719.342130	27.565748
265.086748	8739.100603	27.570765
265.849998	8756.282474	27.575783
266.195394	8764.796791	27.580800
266.261529	8790.254671	27.585818
266.691465	8793.393204	27.590836
266.752224	8796.318707	27.595853
267.208519	8819.650805	27.600871
267.608820	8829.653093	27.605888
267.801695	8841.018314	27.610906
268.015642	8849.908130	27.615924
268.016593	8858.779965	27.620941
268.389498	8879.617196	27.625959
268.678299	8883.081989	27.630976
269.138378	8911.735463	27.635994
269.512320	8913.826527	27.641012
269.680448	8927.104004	27.646029
269.878406	8940.589204	27.651047
270.330293	8944.846008	27.656064
270.634475	8959.375045	27.661082
270.855256	8968.960650	27.666100
271.156493	8992.862276	27.671117
271.620725	8995.601932	27.676135
272.031323	8988.797443	27.681152
271.837895	9011.159661	27.686170
272.412025	9022.878562	27.691188
272.420186	9035.553284	27.696205
272.885892	9034.839742	27.701223
273.023708	9057.235793	27.706240
272.856782	9061.530670	27.711258
273.538537	9080.768343	27.716276
273.263367	9098.124385	27.721293
273.547485	9108.701335	27.726311
273.911446	9123.479113	27.731328
273.950517	9153.135405	27.736346
274.416443	9168.051211	27.741364
274.724853	9198.278460	27.746381
274.925983	9206.970654	27.751399
275.201679	9229.085695	27.756416
275.565229	9246.948791	27.761434
276.111955	9241.308779	27.766452
276.600038	9274.208658	27.771469
276.527649	9281.298638	27.776487
277.524134	9298.641089	27.781504
277.764571	9320.190577	27.786522
277.973963	9317.598956	27.791540
278.032594	9315.168289	27.796557
278.357019	9330.961414	27.801575
278.544202	9339.930547	27.806592
278.561692	9348.289320	27.811610
279.228994	9360.018426	27.816628
279.519992	9371.237781	27.821645
279.618940	9373.992056	27.826663
279.979551	9373.009203	27.831680
280.099679	9392.764491	27.836698
280.287815	9396.612160	27.841716
280.725933	9392.332696	27.846733
280.680368	9418.912332	27.851751
280.730499	9426.906318	27.856768
281.010036	9450.586678	27.861786
281.491033	9448.843735	27.866804
281.677179	9472.890381	27.871821
281.827809	9491.842200	27.876839
282.385332	9500.564326	27.881856
282.408855	9536.601583	27.886874
282.597403	9539.830691	27.891892
283.015179	9559.020559	27.896909
283.208029	9576.596480	27.901927
283.597492	9593.278203	27.906944
283.744496	9620.182021	27.911962
284.099599	9620.199055	27.916980
284.240949	9644.624554	27.921997
284.695367	9678.260185	27.927015
285.463249	9667.739937	27.932032
285.340348	9697.353869	27.937050
285.821619	9701.356356	27.942068
286.210733	9732.080582	27.947085
286.322015	9738.245956	27.952103
286.734293	9754.739290	27.957120
286.791286	9784.251536	27.962138
287.264973	9786.252069	27.967156
287.573630	9808.790423	27.972173
287.453908	9826.221684	27.977191
288.282019	9826.338822	27.982208
288.534635	9850.332198	27.987226
288.622627	9861.106202	27.992244
289.231745	9856.748596	27.997261
289.321915	9887.542822	28.002279
290.043589	9882.025395	28.007296
290.304192	9908.651929	28.012314
290.420118	9920.060140	28.017332
290.842682	9912.397908	28.022349
290.984865	9941.710770	28.027367
291.510880	9941.774147	28.032384
291.361528	9958.682628	28.037402
291.927065	9974.962516	28.042420
292.102853	9988.955457	28.047437
292.095225	9989.962463	28.052455
292.357955	10010.917597	28.057472
292.648715	10036.044714	28.062490
293.029588	10049.830713	28.067508
293.392259	10059.284230	28.072525
293.479866	10084.147907	28.077543
293.651327	10087.516002	28.082560
294.021260	10103.153561	28.087578
294.618517	10118.032862	28.092596
294.963593	10138.197525	28.097613
295.037721	10149.118748	28.102631
295.585800	10158.735980	28.107648
295.447087	10179.156445	28.112666
295.984570	10175.372852	28.117684
296.602988	10190.116642	28.122701
296.741331	10194.573701	28.127719
296.947844	10201.300153	28.132736
297.242701	10228.827602	28.137754
297.419959	10222.191965	28.142772
298.081107	10249.532404	28.147789
297.911949	10258.388501	28.152807
298.584413	10264.904966	28.157824
298.528503	10296.106962	28.162842
298.809674	10295.278765	28.167860
298.850677	10310.977622	28.172877
298.938550	10326.853179	28.177895
299.379860	10344.838195	28.182912
299.560769	10370.725503	28.187930
299.989854	10392.506172	28.192948
300.109114	10409.924810	28.197965
300.376435	10447.271926	28.202983
301.042789	10449.563331	28.208000
301.483898	10475.228736	28.213018
302.145962	10488.938453	28.218036
302.567354	10507.658738	28.223053
302.551887	10508.268024	28.228071
303.120484	10533.490991	28.233088
303.139931	10543.802247	28.238106
303.469643	10554.138827	28.243124
303.571757	10561.944912	28.248141
304.184321	10579.477940	28.253159
304.690785	10584.696100	28.258176
304.624198	10592.791550	28.263194
305.160022	10616.131095	28.268212
305.720542	10621.694801	28.273229
305.653907	10636.000069	28.278247
305.855445	10655.197082	28.283264
306.169898	10667.796822	28.288282
306.428822	10682.289496	28.293300
306.963042	10694.566191	28.298317
307.165968	10715.346502	28.303335
307.270250	10721.099828	28.308352
307.631340	10744.058573	28.313370
307.898675	10759.314946	28.318388
308.155033	10769.107741	28.323405
308.301528	10791.920143	28.328423
308.804086	10798.171551	28.333440
309.161327	10826.968644	28.338458
309.603355	10834.098962	28.343476
310.132787	10852.423909	28.348493
310.507168	10868.760816	28.353511
310.723979	10872.194267	28.358528
310.983320	10894.661838	28.363546
311.305030	10904.878736	28.368564
311.583552	10905.652497	28.373581
311.913768	10927.533910	28.378599
311.932746	10932.419853	28.383616
312.032585	10943.684234	28.388634
312.274697	10954.205440	28.393652
312.552506	10976.931085	28.398669
312.319873	11003.368812	28.403687
313.460568	11019.917843	28.408704
313.931865	11028.144626	28.413722
313.694056	11051.372824	28.418740
314.314162	11064.918976	28.423757
314.357593	11080.630841	28.428775
314.967665	11105.702169	28.433792
315.021904	11113.632649	28.438810
315.324221	11134.833709	28.443828
316.049860	11143.170736	28.448845
316.158554	11180.306090	28.453863
316.770467	11191.552403	28.458880
316.625500	11209.140000	28.463898
316.928832	11225.126979	28.468916
317.387854	11247.061524	28.473933
317.666051	11269.216559	28.478951
318.118538	11290.007080	28.483968
318.397277	11301.522614	28.488986
318.744561	11314.757914	28.494004
319.243046	11339.519224	28.499021
319.338237	11352.924594	28.504039
320.043210	11355.777839	28.509056
320.133617	11381.342883	28.514074
320.225248	11403.824955	28.519092
320.786926	11404.052670	28.524109
320.837536	11433.444812	28.529127
321.402679	11454.205014	28.534144
321.598809	11466.903379	28.539162
321.958216	11498.614638	28.544180
322.456949	11497.239739	28.549197
322.339069	11525.339437	28.554215
322.748616	11544.921961	28.559232
323.190306	11539.132572	28.564250
323.620160	11578.286859	28.569268
324.362697	11577.050972	28.574285
324.029412	11600.047701	28.579303
324.934245	11607.043246	28.584320
325.087598	11639.140628	28.589338
325.488686	11651.911164	28.594356
326.189860	11656.889713	28.599373
326.226028	11668.880604	28.604391
326.580660	11679.610270	28.609408
326.800714	11700.270365	28.614426
327.123465	11718.793409	28.619444
327.256737	11728.528134	28.624461
327.343875	11743.093676	28.629479
327.843850	11753.372862	28.634496
327.970337	11781.983457	28.639514
328.217474	11789.849314	28.644532
328.876851	11810.298271	28.649549
328.979936	11822.802406	28.654567
329.110577	11832.844965	28.659584
329.692323	11850.604573	28.664602
329.759099	11873.926179	28.669620
330.307721	11891.542557	28.674637
330.843996	11915.592602	28.679655
330.994684	11927.183132	28.684672
331.528341	11947.837468	28.689690
331.487341	11967.483487	28.694708
332.263901	11966.334042	28.699725
332.230067	11988.627815	28.704743
332.715329	12022.456217	28.709760
333.106695	12027.893147	28.714778
333.125816	12044.845585	28.719796
333.407154	12056.157628	28.724813
333.584154	12089.275585	28.729831
333.999136	12096.996795	28.734848
334.430508	12126.542113	28.739866
334.626968	12143.682846	28.744884
335.549240	12163.659466	28.749901
335.649738	12185.004355	28.754919
335.908386	12202.463849	28.759936
336.508383	12208.580296	28.764954
336.701288	12238.480242	28.769972
337.171557	12252.077518	28.774989
337.430820	12278.433175	28.780007
337.836219	12289.643373	28.785024
338.314749	12303.008370	28.790042
338.161652	12325.514283	28.795060
338.913822	12336.822933	28.800077
338.742849	12363.083389	28.805095
339.283117	12382.365967	28.810112
340.121596	12402.887739	28.815130
340.209157	12411.915710	28.820148
340.522328	12437.639482	28.825165
340.881714	12453.504704	28.830183
341.041728	12479.225406	28.835200
341.347545	12489.081098	28.840218
341.394913	12522.175007	28.845236
342.158165	12532.683729	28.850253
342.552655	12562.901267	28.855271
342.652839	12569.997755	28.860288
343.205886	12582.221248	28.865306
343.355004	12613.404795	28.870324
343.997470	12621.532767	28.875341
344.202039	12657.107848	28.880359
344.386096	12653.773335	28.885376
344.957330	12686.340982	28.890394
345.322931	12707.543218	28.895412
345.719827	12714.484460	28.900429
345.915622	12733.889286	28.905447
346.146576	12761.417178	28.910464
346.458543	12770.568991	28.915482
346.694872	12788.726947	28.920500
346.880578	12818.507574	28.925517
347.306646	12837.740454	28.930535
347.844037	12844.246922	28.935552
348.493883	12863.328666	28.940570
348.389543	12891.757944	28.945588
348.958189	12904.944019	28.950605
348.976946	12922.453001	28.955623
349.761329	12946.447834	28.960640
350.389096	12957.249805	28.965658
350.198271	12984.097749	28.970676
350.624819	12989.112251	28.975693
351.236556	13013.155955	28.980711
351.614686	13026.455340	28.985728
352.070213	13034.232361	28.990746
352.088630	13063.309679	28.995764
352.312249	13073.726099	29.000781
352.430750	13093.603578	29.005799
352.722332	13117.702599	29.010816
353.208820	13136.287282	29.015834
353.643001	13157.995378	29.020852
353.700492	13183.128899	29.025869
354.261703	13207.615459	29.030887
354.541261	13243.800221	29.035904
355.247456	13257.376355	29.040922
355.053028	13278.621208	29.045940
355.768473	13306.430438	29.050957
356.186742	13332.614213	29.055975
356.735909	13345.894692	29.060992
357.126718	13369.480043	29.066010
357.259512	13397.180778	29.071028
357.974372	13402.563315	29.076045
358.138494	13427.007439	29.081063
358.738832	13456.097664	29.086080
359.285818	13471.472991	29.091098
359.299005	13492.512968	29.096116
359.758042	13506.065642	29.101133
360.304807	13513.185176	29.106151
360.121020	13537.945562	29.111168
360.472565	13569.460703	29.116186
360.631812	13575.508132	29.121204
361.267693	13593.745265	29.126221
361.827202	13615.950810	29.131239
362.261191	13639.222513	29.136256
362.860034	13663.240180	29.141274
362.792931	13673.304842	29.146292
363.483105	13689.119239	29.151309
363.646151	13716.433178	29.156327
364.154651	13725.064543	29.161344
364.734324	13748.668306	29.166362
364.647668	13765.022779	29.171380
365.009225	13782.618043	29.176397
365.623325	13783.538528	29.181415
365.717360	13819.628080	29.186432
366.165767	13824.760111	29.191450
366.193950	13866.063995	29.196468
366.832432	13876.719220	29.201485
367.021908	13897.152213	29.206503
366.952635	13916.641621	29.211520
367.457374	13937.132174	29.216538
367.803625	13955.824436	29.221556
368.565203	13985.075458	29.226573
368.789543	14003.041656	29.231591
368.931884	14027.350983	29.236608
369.718325	14048.414630	29.241626
369.906728	14060.656004	29.246644
370.466098	14095.412285	29.251661
370.837808	14105.017459	29.256679
370.770793	14129.680198	29.261696
371.336306	14150.221968	29.266714
371.735068	14165.511709	29.271732
372.269393	14180.505139	29.276749
372.527608	14207.334354	29.281767
372.943387	14225.094571	29.286784
373.678249	14245.746061	29.291802
373.481549	14276.534504	29.296820
373.952000	14285.152377	29.301837
374.288360	14311.490321	29.306855
374.501602	14348.743499	29.311872
375.239010	14354.496311	29.316890
375.415427	14393.508535	29.321908
376.041648	14405.616266	29.326925
376.571657	14427.176691	29.331943
376.741462	14454.102885	29.336960
377.156145	14471.088080	29.341978
377.609242	14490.053463	29.346996
377.918615	14505.710947	29.352013
378.476765	14520.263334	29.357031
378.674656	14548.853389	29.362048
379.265247	14557.245143	29.367066
379.507359	14587.616151	29.372084
380.008015	14610.684870	29.377101
380.365665	14624.441070	29.382119
380.363942	14636.145039	29.387136
381.404603	14654.113294	29.392154
381.244827	14670.701098	29.397172
381.682120	14696.440969	29.402189
382.319836	14712.057661	29.407207
382.642077	14734.028700	29.412224
383.055291	14759.410422	29.417242
383.478841	14781.417342	29.422260
383.742955	14796.888879	29.427277
383.989679	14826.426462	29.432295
384.438160	14851.196170	29.437312
384.517969	14860.964252	29.442330
385.277231	14897.562411	29.447348
385.415689	14906.906412	29.452365
385.765662	14933.545453	29.457383
385.973000	14960.122937	29.462400
387.029310	14986.387575	29.467418
387.237536	15000.568522	29.472436
387.244743	15009.797802	29.477453
387.767152	15029.433761	29.482471
387.863526	15062.011314	29.487488
388.355118	15065.700597	29.492506
388.617083	15090.584548	29.497524
388.958299	15108.397234	29.502541
389.771240	15125.119941	29.507559
390.093200	15142.633243	29.512576
390.610755	15165.955566	29.517594
390.912639	15194.237703	29.522612
391.046236	15207.270451	29.527629
391.410621	15235.434855	29.532647
391.714076	15250.284867	29.537664
392.671767	15270.044751	29.542682
393.128470	15279.946313	29.547700
393.126484	15309.247842	29.552717
393.714430	15325.432035	29.557735
394.138469	15341.839073	29.562752
394.553768	15376.404443	29.567770
394.689704	15396.952872	29.572788
395.318413	15412.806222	29.577805
395.885623	15429.715240	29.582823
395.941030	15455.586048	29.587840
396.344380	15476.327263	29.592858
396.693840	15493.963136	29.597876
396.820024	15526.835784	29.602893
397.260775	15546.190005	29.607911
397.805074	15572.031330	29.612928
398.376852	15601.690531	29.617946
398.663609	15632.038883	29.622964
399.167150	15649.623519	29.627981
399.661152	15668.154010	29.632999
399.908641	15695.354110	29.638016
400.546348	15711.124855	29.643034
400.905163	15741.630710	29.648052
401.449676	15747.515174	29.653069
402.032620	15776.252529	29.658087
402.244156	15789.142669	29.663104
402.688164	15812.189755	29.668122
402.997860	15831.136356	29.673140
402.997504	15860.426079	29.678157
403.719989	15879.212201	29.683175
403.517580	15901.391028	29.688192
404.075920	15926.881858	29.693210
405.158178	15947.227103	29.698228
405.241015	15976.998788	29.703245
405.594417	15989.928588	29.708263
406.022911	16022.986867	29.713280
406.478208	16035.092334	29.718298
406.818672	16066.403598	29.723316
406.904911	16097.163399	29.728333
407.822217	16111.948819	29.733351
408.182536	16148.807405	29.738368
408.531225	16156.607193	29.743386
409.064763	16165.657849	29.748404
409.089291	16187.957697	29.753421
409.565036	16207.180623	29.758439
409.785366	16236.251477	29.763456
409.851802	16251.566442	29.768474
410.372305	16279.146455	29.773492
410.570290	16308.904962	29.778509
411.315398	16331.561990	29.783527
411.902400	16359.134898	29.788544
412.405603	16380.998769	29.793562
413.164843	16392.088312	29.798580
413.357318	16426.516377	29.803597
413.806450	16434.489845	29.808615
414.264624	16470.535097	29.813632
414.825428	16473.937657	29.818650
415.028012	16506.566693	29.823668
415.385573	16518.151768	29.828685
415.829686	16541.110378	29.833703
415.968483	16564.735109	29.838720
416.016969	16594.966357	29.843738
416.900882	16610.075851	29.848756
417.089821	16658.470010	29.853773
417.757677	16680.292721	29.858791
417.871914	16701.816511	29.863808
418.524869	16720.422349	29.868826
418.742895	16761.608509	29.873844
419.462742	16782.070481	29.878861
420.074384	16810.452977	29.883879
420.183631	16839.542077	29.888896
420.782865	16856.015532	29.893914
421.662157	16883.090695	29.898932
421.377248	16914.740699	29.903949
421.914245	16930.918868	29.908967
422.436532	16965.701846	29.913984
422.386723	16988.835675	29.919002
423.194286	17018.945632	29.924020
423.610832	17051.771040	29.929037
424.079815	17075.181757	29.934055
424.681305	17104.236822	29.939072
424.746256	17137.787071	29.944090
425.370358	17165.761581	29.949108
425.668212	17191.679246	29.954125
426.369437	17223.215873	29.959143
426.431617	17240.078430	29.964160
427.111888	17264.052769	29.969178
427.543163	17293.012091	29.974196
427.897867	17316.350838	29.979213
428.777072	17343.633307	29.984231
429.123652	17360.857543	29.989248
429.516691	17374.040051	29.994266
430.098987	17401.499051	29.999284
430.432472	17425.053532	30.004301
430.696451	17440.881670	30.009319
431.058770	17469.899552	30.014336
431.374342	17483.737168	30.019354
431.732886	17507.419270	30.024372
431.888659	17543.439426	30.029389
432.716483	17556.461093	30.034407
432.974793	17577.200007	30.039424
433.251162	17608.667127	30.044442
434.292279	17621.687150	30.049460
434.252858	17651.194156	30.054477
434.672531	17675.652756	30.059495
434.788248	17692.502749	30.064512
435.247066	17736.292372	30.069530
435.818712	17752.897755	30.074548
436.334430	17791.578330	30.079565
436.636591	17808.554250	30.084583
436.898162	17842.796124	30.089600
437.038763	17874.783425	30.094618
437.785526	17903.772760	30.099636
438.091752	17941.628065	30.104653
438.607587	17972.773533	30.109671
439.144200	18001.932355	30.114688
439.685809	18025.981545	30.119706
440.095072	18052.724216	30.124724
440.490312	18081.054949	30.129741
440.982583	18117.200776	30.134759
441.712953	18151.401714	30.139776
442.072921	18172.971076	30.144794
442.868848	18193.872207	30.149812
443.254682	18227.865218	30.154829
443.648437	18253.547342	30.159847
444.466754	18288.461724	30.164864
444.932258	18307.430642	30.169882
445.366201	18312.781170	30.174900
445.291025	18346.077818	30.179917
445.703213	18365.958835	30.184935
446.297337	18392.816342	30.189952
446.608464	18414.676497	30.194970
447.067650	18443.230775	30.199988
447.519301	18477.059516	30.205005
448.378808	18495.071409	30.210023
448.676035	18523.254787	30.215040
449.226172	18554.106984	30.220058
449.762110	18578.214236	30.225076
449.647079	18609.220544	30.230093
450.189018	18623.009141	30.235111
450.551427	18664.265155	30.240128
450.835393	18702.717994	30.245146
451.752098	18722.582086	30.250164
452.024963	18755.736759	30.255181
452.300370	18776.439712	30.260199
452.741623	18803.933321	30.265216
453.275324	18847.427532	30.270234
453.818398	18864.433948	30.275252
454.431579	18894.427941	30.280269
454.783077	18925.200707	30.285287
455.614383	18934.401636	30.290304
455.695672	18969.035747	30.295322
456.126141	18979.706113	30.300340
456.485790	19004.280708	30.305357
456.862936	19034.298401	30.310375
457.426094	19057.767002	30.315392
457.530768	19090.154668	30.320410
458.341655	19113.114579	30.325428
458.275815	19143.318019	30.330445
458.784669	19181.482268	30.335463
459.458401	19203.338919	30.340480
459.406721	19244.040364	30.345498
460.422869	19266.949299	30.350516
460.603953	19307.697297	30.355533
461.320071	19336.629630	30.360551
462.086075	19363.722869	30.365568
462.231700	19396.748777	30.370586
463.052657	19410.642061	30.375604
463.327188	19448.686806	30.380621
463.667124	19468.749261	30.385639
464.201790	19491.189530	30.390656
464.443978	19530.311740	30.395674
464.963373	19545.170175	30.400692
465.231510	19597.825137	30.405709
465.515661	19628.675776	30.410727
466.197667	19667.549117	30.415744
466.585184	19719.999238	30.420762
467.472217	19738.289322	30.425780
467.591276	19777.165210	30.430797
468.029205	19807.319602	30.435815
468.830676	19844.647851	30.440832
469.466780	19874.436917	30.445850
470.110212	19902.960194	30.450868
470.556547	19940.056244	30.455885
471.139132	19948.933594	30.460903
471.528060	19975.918271	30.465920
472.058384	20008.675507	30.470938
472.731204	20030.792549	30.475956
473.071355	20065.317375	30.480973
473.340699	20089.133582	30.485991
474.182872	20107.863184	30.491008
474.223663	20146.113809	30.496026
474.864047	20164.542125	30.501044
475.010360	20203.926202	30.506061
475.516062	20222.390217	30.511079
475.937711	20257.587205	30.516096
476.459537	20287.270842	30.521114
477.232916	20318.079557	30.526132
477.516783	20349.404553	30.531149
477.982305	20382.052803	30.536167
478.622571	20410.522784	30.541184
478.760597	20437.887639	30.546202
479.345442	20470.438316	30.551220
479.854429	20509.764206	30.556237
480.239418	20525.549830	30.561255
480.691836	20562.090018	30.566272
480.898182	20594.111407	30.571290
481.457057	20619.316741	30.576308
481.907300	20646.867689	30.581325
482.242090	20685.866999	30.586343
482.936548	20704.783867	30.591360
483.480185	20750.632919	30.596378
483.896047	20771.285040	30.601396
484.424418	20809.541907	30.606413
485.162621	20833.490101	30.611431
485.605429	20857.575952	30.616448
486.113345	20887.499595	30.621466
486.784031	20911.736660	30.626484
486.982036	20936.743654	30.631501
487.272478	20982.725859	30.636519
487.929316	21000.909200	30.641536
488.531964	21039.741504	30.646554
489.045657	21058.472996	30.651572
489.173505	21102.507118	30.656589
489.710051	21118.577124	30.661607
490.265547	21152.649501	30.666624
490.467078	21187.074451	30.671642
491.006148	21233.747831	30.676660
491.664609	21255.649177	30.681677
491.974374	21315.396251	30.686695
492.640655	21337.750090	30.691712
492.771545	21382.097952	30.696730
493.539714	21408.661630	30.701748
493.939966	21440.724343	30.706765
494.768515	21487.679985	30.711783
495.452276	21519.221228	30.716800
495.542773	21548.559745	30.721818
496.153936	21589.297933	30.726836
496.721591	21628.349909	30.731853
497.425619	21648.869471	30.736871
497.825324	21684.238939	30.741888
498.029855	21723.971956	30.746906
499.022405	21753.601898	30.751924
499.309664	21794.619033	30.756941
499.863653	21822.435896	30.761959
500.742787	21856.735473	30.766976
500.784343	21890.158091	30.771994
501.205779	21923.353303	30.777012
502.028744	21967.780013	30.782029
502.357626	21992.457535	30.787047
503.039633	22030.407802	30.792064
503.420297	22054.084824	30.797082
504.009007	22087.103309	30.802100
504.393483	22118.532764	30.807117
504.829934	22168.337001	30.812135
505.163014	22190.353704	30.817152
505.632123	22233.709709	30.822170
506.152177	22261.350821	30.827188
506.666179	22296.934223	30.832205
507.121531	22332.866499	30.837223
507.882654	22361.632662	30.842240
508.305752	22392.346102	30.847258
508.948613	22433.102691	30.852276
509.227203	22459.013669	30.857293
510.018880	22498.059685	30.862311
510.681769	22506.025483	30.867328
510.752934	22546.233110	30.872346
510.923221	22578.871917	30.877364
512.025618	22600.824146	30.882381
512.415515	22644.979930	30.887399
512.865061	22668.839081	30.892416
513.294101	22705.330087	30.897434
513.854915	22729.047951	30.902452
514.048934	22765.081122	30.907469
514.867949	22794.719409	30.912487
515.191868	22839.265876	30.917504
515.755009	22876.683422	30.922522
516.482452	22907.379316	30.927540
517.033157	22941.516979	30.932557
517.587398	22965.382743	30.937575
518.093582	22996.900892	30.942592
518.685608	23037.296956	30.947610
519.155782	23074.200493	30.952628
519.486561	23096.074691	30.957645
519.989640	23132.308361	30.962663
520.657801	23161.874490	30.967680
520.914814	23211.911445	30.972698
521.359063	23243.844009	30.977716
522.187767	23284.696856	30.982733
522.839049	23309.115572	30.987751
523.410951	23352.985208	30.992768
523.479980	23392.754243	30.997786
524.113516	23417.020787	31.002804
524.779338	23457.540858	31.007821
525.282065	23509.097582	31.012839
526.020801	23530.144166	31.017856
526.434961	23572.034173	31.022874
526.739720	23614.918409	31.027892
527.389984	23643.375331	31.032909
527.511009	23686.751382	31.037927
528.354315	23725.215644	31.042944
528.935747	23768.212184	31.047962
529.129108	23802.821359	31.052980
529.865924	23834.189442	31.057997
530.086989	23893.226282	31.063015
530.850652	23926.963522	31.068032
531.352621	23976.017875	31.073050
531.799230	24013.040777	31.078068
532.599804	24052.351515	31.083085
533.030233	24100.369248	31.088103
533.760380	24134.499020	31.093120
534.192153	24178.026198	31.098138
534.934342	24217.285994	31.103156
535.658316	24250.947539	31.108173
535.779794	24288.733364	31.113191
536.651161	24313.049259	31.118208
537.336482	24367.168826	31.123226
537.692368	24389.198349	31.128244
538.417530	24413.704678	31.133261
538.755514	24439.498371	31.138279
539.280560	24477.002171	31.143296
539.588371	24500.555039	31.148314
540.302053	24525.255568	31.153332
540.690101	24560.055151	31.158349
540.640008	24604.476307	31.163367
541.231449	24631.166522	31.168384
542.167950	24683.517356	31.173402
542.431751	24723.342978	31.178420
543.378522	24745.390736	31.183437
543.597672	24799.992485	31.188455
544.319892	24831.468056	31.193472
544.799037	24872.146720	31.198490
545.297791	24918.781471	31.203508
545.920376	24948.738664	31.208525
546.402707	24998.127776	31.213543
546.927690	25030.857706	31.218560
547.680333	25074.069189	31.223578
547.853962	25118.946109	31.228596
548.414472	25154.428479	31.233613
549.145951	25197.745286	31.238631
549.382564	25248.042392	31.243648
550.295938	25290.024411	31.248666
550.857387	25335.170231	31.253684
551.334932	25372.163009	31.258701
551.686972	25425.906783	31.263719
552.587871	25449.920378	31.268736
553.252471	25501.135585	31.273754
553.785214	25547.980241	31.278772
554.365552	25571.909582	31.283789
554.962506	25622.321415	31.288807
555.360004	25661.322996	31.293824
556.091941	25695.398327	31.298842
556.392709	25740.755393	31.303860
557.202454	25768.870893	31.308877
557.338282	25823.078981	31.313895
557.675442	25874.798925	31.318912
558.262981	25908.754337	31.323930
559.000371	25967.801692	31.328948
560.019616	26008.142778	31.333965
560.185468	26053.763276	31.338983
560.843760	26097.380143	31.344000
561.721808	26138.896568	31.349018
562.324788	26172.853232	31.354036
563.251019	26207.799148	31.359053
563.782086	26247.410323	31.364071
564.212838	26275.428732	31.369088
564.862458	26305.157285	31.374106
565.316024	26340.434802	31.379124
565.997113	26372.922827	31.384141
566.529670	26423.823267	31.389159
567.026148	26448.212382	31.394176
567.214317	26489.555985	31.399194
567.788545	26531.447177	31.404212
568.446745	26564.194482	31.409229
568.602775	26598.886562	31.414247
569.134239	26629.319924	31.419264
570.076094	26672.650553	31.424282
570.504827	26716.062233	31.429300
571.200983	26749.134751	31.434317
571.715589	26775.606025	31.439335
572.113891	26813.471893	31.444352
572.625654	26861.478666	31.449370
572.904236	26897.463586	31.454388
573.846453	26934.137017	31.459405
574.171172	26994.939024	31.464423
574.486721	27026.581383	31.469440
575.155598	27072.728133	31.474458
575.906542	27127.384680	31.479476
576.263299	27180.244908	31.484493
576.781405	27223.587788	31.489511
577.179281	27280.576348	31.494528
577.870182	27326.587963	31.499546
578.646314	27373.860075	31.504564
579.407192	27425.800365	31.509581
580.047163	27476.420739	31.514599
580.844674	27507.312889	31.519616
581.740822	27553.601302	31.524634
582.003657	27597.486915	31.529652
582.697924	27637.210249	31.534669
583.576938	27675.035464	31.539687
584.036847	27732.792569	31.544704
584.839877	27762.742053	31.549722
584.961124	27807.114046	31.554740
585.588685	27851.977517	31.559757
585.945525	27897.375856	31.564775
586.541393	27950.900154	31.569792
587.035705	27982.381981	31.574810
587.673017	28026.020032	31.579828
588.395204	28069.004929	31.584845
588.932306	28110.709965	31.589863
589.725535	28162.938205	31.594880
590.418590	28208.253934	31.599898
590.780048	28256.518860	31.604916
591.651115	28289.249174	31.609933
592.000472	28338.631918	31.614951
592.736972	28382.113315	31.619968
593.482798	28423.774889	31.624986
593.976227	28476.322922	31.630004
594.404947	28505.120039	31.635021
594.929796	28562.969043	31.640039
595.591805	28602.466673	31.645056
596.051250	28643.774167	31.650074
596.562684	28694.892361	31.655092
597.382534	28738.849946	31.660109
597.702761	28790.564610	31.665127
598.466734	28845.376180	31.670144
599.118763	28875.416388	31.675162
599.893933	28925.579329	31.680180
600.697235	28970.034989	31.685197
600.660261	29005.637562	31.690215
601.706686	29028.687853	31.695232
602.786379	29061.632343	31.700250
603.029395	29114.702957	31.705268
603.705339	29133.152604	31.710285
604.015340	29168.397714	31.715303
604.345433	29217.494669	31.720320
604.908791	29247.822315	31.725338
605.552958	29297.208306	31.730356
606.113923	29344.704042	31.735373
606.767799	29381.850513	31.740391
607.361388	29440.213315	31.745408
607.818942	29491.835852	31.750426
607.972073	29543.306893	31.755444
609.269662	29579.629549	31.760461
609.795328	29631.416608	31.765479
610.096136	29684.306528	31.770496
611.144139	29724.771341	31.775514
611.508769	29776.940662	31.780532
612.393160	29813.079072	31.785549
612.803779	29858.326200	31.790567
613.331044	29916.327778	31.795584
614.094671	29955.815675	31.800602
614.523787	30016.112037	31.805620
615.544604	30069.523653	31.810637
616.277363	30118.887001	31.815655
616.568496	30158.160658	31.820672
617.348505	30204.848655	31.825690
618.005603	30254.430913	31.830708
618.872408	30291.444695	31.835725
619.372052	30348.268659	31.840743
619.694756	30392.631390	31.845760
620.737319	30425.463220	31.850778
621.033108	30471.234647	31.855796
621.915591	30521.442164	31.860813
622.531546	30562.026720	31.865831
622.844011	30620.684373	31.870848
623.688647	30666.728276	31.875866
624.165592	30727.211921	31.880884
624.882504	30762.517036	31.885901
625.193081	30820.353027	31.890919
625.678230	30870.877053	31.895936
626.559506	30915.580935	31.900954
626.949842	30970.712906	31.905972
627.561133	31019.634970	31.910989
628.570896	31071.497661	31.916007
629.133549	31120.289080	31.921024
629.978992	31168.866976	31.926042
630.702454	31216.449462	31.931060
631.407245	31260.331321	31.936077
631.878089	31310.416110	31.941095
632.378796	31362.020354	31.946112
633.600187	31394.803600	31.951130
633.952584	31437.307824	31.956148
634.414865	31468.385425	31.961165
634.768497	31512.713170	31.966183
634.901556	31560.198387	31.971200
635.632151	31595.786820	31.976218
636.203577	31651.026212	31.981236
636.909455	31699.462417	31.986253
637.621046	31746.632244	31.991271
638.390310	31801.188130	31.996288
639.413758	31838.604456	32.001306
639.684733	31896.199945	32.006324
640.465230	31938.678279	32.011341
641.188637	32001.206287	32.016359
641.813400	32032.285878	32.021376
642.420390	32085.374376	32.026394
642.710455	32142.362451	32.031412
643.637903	32184.981942	32.036429
643.975572	32235.078149	32.041447
644.619444	32295.069727	32.046464
645.033508	32338.958211	32.051482
645.760764	32412.925382	32.056500
646.453160	32452.334511	32.061517
647.397864	32514.389481	32.066535
647.993557	32576.022675	32.071552
648.531238	32618.478384	32.076570
649.106959	32682.071204	32.081588
649.661695	32734.386748	32.086605
650.070755	32788.344415	32.091623
650.556413	32850.558861	32.096640
651.782100	32911.563389	32.101658
652.306683	32965.273113	32.106676
653.061261	33024.989644	32.111693
653.750742	33094.725839	32.116711
654.546558	33148.593153	32.121728
655.097954	33197.390956	32.126746
656.177307	33259.857609	32.131764
657.070534	33305.243890	32.136781
657.743983	33358.685296	32.141799
657.901902	33409.168347	32.146816
658.881050	33447.479679	32.151834
659.463978	33503.921418	32.156852
660.086393	33560.853589	32.161869
661.223812	33588.336241	32.166887
661.918420	33656.527660	32.171904
662.517413	33699.729854	32.176922
663.336320	33745.777038	32.181940
664.012705	33791.129826	32.186957
665.340357	33814.782109	32.191975
665.525466	33872.090785	32.196992
666.114087	33906.415832	32.202010
666.859307	33944.741923	32.207028
667.520542	33993.382719	32.212045
668.007982	34030.846823	32.217063
668.492155	34067.108795	32.222080
669.045855	34110.049722	32.227098
669.794321	34153.333339	32.232116
670.332991	34193.204599	32.237133
670.797899	34231.587021	32.242151
671.197299	34281.826203	32.247168
671.890253	34326.760090	32.252186
672.640973	34383.887471	32.257204
673.024014	34429.378567	32.262221
673.686960	34474.246696	32.267239
674.439692	34529.574050	32.272256
675.023484	34586.050866	32.277274
675.489815	34643.233878	32.282292
676.126454	34695.972937	32.287309
676.806768	34751.482810	32.292327
677.384825	34814.205401	32.297344
678.133086	34873.880741	32.302362
678.832348	34931.475356	32.307380
679.499640	34996.889544	32.312397
680.095728	35052.010269	32.317415
680.835661	35114.478061	32.322432
681.636503	35178.232216	32.327450
682.127817	35240.689619	32.332468
682.479303	35286.024132	32.337485
683.460500	35353.532126	32.342503
684.381303	35417.759950	32.347520
685.058749	35476.455559	32.352538
685.986197	35535.557711	32.357556
686.535416	35600.182763	32.362573
687.302216	35660.170111	32.367591
687.779710	35726.366207	32.372608
688.847830	35774.274275	32.377626
689.584831	35833.879175	32.382644
690.286047	35898.462264	32.387661
691.141091	35946.671182	32.392679
691.580535	36006.521136	32.397696
692.700241	36060.038918	32.402714
693.620659	36115.106790	32.407732
694.013352	36168.237758	32.412749
694.452797	36225.638577	32.417767
695.146101	36286.246839	32.422784
696.015719	36328.430596	32.427802
696.518441	36398.319168	32.432820
697.177269	36445.925419	32.437837
698.212007	36497.745998	32.442855
698.689249	36568.085500	32.447872
699.679079	36609.164576	32.452890
700.552936	36665.904953	32.457908
700.964376	36725.143918	32.462925
701.766157	36765.510750	32.467943
702.252854	36833.860217	32.472960
702.971526	36875.799791	32.477978
703.445649	36944.738203	32.482996
704.316352	37005.066990	32.488013
705.285549	37056.543423	32.493031
706.043385	37115.515775	32.498048
706.990805	37159.373065	32.503066
707.641283	37203.708164	32.508084
707.605300	37251.335877	32.513101
708.614499	37308.736408	32.518119
709.072391	37348.121970	32.523136
709.535121	37408.499816	32.528154
710.056483	37456.390967	32.533172
710.664119	37520.101246	32.538189
711.802896	37574.538449	32.543207
712.330782	37640.882285	32.548224
713.199880	37691.424298	32.553242
713.950272	37744.508037	32.558260
714.350370	37796.373756	32.563277
715.204888	37857.944298	32.568295
715.871154	37923.988146	32.573312
716.560638	37980.718172	32.578330
717.188920	38046.446900	32.583348
717.905799	38112.169663	32.588365
718.705707	38175.244777	32.593383
719.511881	38249.769264	32.598400
720.051232	38312.339249	32.603418
720.961946	38365.178679	32.608436
721.468958	38431.191525	32.613453
722.439126	38502.335724	32.618471
722.946266	38565.703300	32.623488
723.848604	38628.801644	32.628506
724.533747	38687.251823	32.633524
725.131816	38771.727989	32.638541
726.134644	38819.294079	32.643559
727.022675	38897.947420	32.648576
727.686707	38966.244186	32.653594
728.488945	39003.718187	32.658612
728.947673	39078.897667	32.663629
729.960722	39134.424265	32.668647
730.680947	39208.739601	32.673664
731.618508	39260.431217	32.678682
732.399134	39340.541767	32.683700
732.921057	39393.890971	32.688717
733.872237	39452.068068	32.693735
734.485466	39509.950683	32.698752
735.092743	39579.320165	32.703770
735.746177	39647.730166	32.708788
736.636641	39701.866859	32.713805
737.638329	39758.691911	32.718823
737.808528	39838.782146	32.723840
738.574803	39895.126341	32.728858
739.447041	39974.446321	32.733876
739.935191	40027.282520	32.738893
741.357882	40083.041893	32.743911
741.863964	40155.523693	32.748928
742.411342	40209.781275	32.753946
743.345147	40268.530044	32.758964
743.939891	40343.408043	32.763981
744.999818	40404.459998	32.768999
746.096090	40464.653271	32.774016
746.876267	40519.720014	32.779034
747.320758	40564.847337	32.784052
747.660525	40629.463497	32.789069
748.685254	40669.988682	32.794087
749.127540	40724.625754	32.799104
749.981867	40781.928692	32.804122
750.450984	40839.031369	32.809140
751.351102	40894.715745	32.814157
751.854041	40947.388438	32.819175
752.421876	41006.440864	32.824192
753.480901	41076.359550	32.829210
754.259336	41130.442929	32.834228
754.770730	41215.900680	32.839245
755.364421	41259.202007	32.844263
756.138097	41346.381742	32.849280
756.695189	41404.497357	32.854298
757.620042	41478.204949	32.859316
758.235849	41548.379054	32.864333
758.767793	41621.206746	32.869351
759.707488	41702.015890	32.874368
760.467373	41768.250596	32.879386
761.399363	41845.970637	32.884404
762.138672	41918.760276	32.889421
763.116430	41988.749247	32.894439
763.858322	42052.713788	32.899456
764.655697	42132.402662	32.904474
765.500953	42193.758559	32.909492
766.138558	42272.852145	32.914509
767.351471	42329.071769	32.919527
768.288217	42414.448856	32.924544
768.821610	42466.670318	32.929562
769.715005	42546.295360	32.934580
770.456644	42623.024094	32.939597
771.316652	42681.799212	32.944615
772.232886	42758.879271	32.949632
772.767054	42809.953497	32.954650
773.552331	42871.103715	32.959668
774.249331	42946.509885	32.964685
775.085417	43004.611738	32.969703
775.743417	43079.986848	32.974720
776.615073	43135.954310	32.979738
777.742836	43210.460322	32.984756
778.247101	43279.772874	32.989773
779.437296	43339.790971	32.994791
780.070550	43408.342229	32.999808
780.761982	43471.298053	33.004826
781.635746	43524.124657	33.009844
782.176421	43598.669016	33.014861
783.193664	43659.589532	33.019879
783.628067	43730.063225	33.024896
784.355985	43809.228345	33.029914
785.604226	43875.027506	33.034932
785.917128	43938.628862	33.039949
786.855227	44016.013886	33.044967
787.843183	44073.316003	33.049984
788.620560	44136.724283	33.055002
789.555457	44196.814389	33.060020
790.065201	44249.278444	33.065037
790.878876	44308.230515	33.070055
791.571530	44355.874013	33.075072
792.129438	44424.091131	33.080090
793.563286	44481.096497	33.085108
793.697310	44547.141813	33.090125
794.190420	44617.442574	33.095143
795.417413	44661.367752	33.100160
796.074234	44739.930134	33.105178
797.037230	44800.658252	33.110196
797.374063	44873.641134	33.115213
798.066390	44931.693479	33.120231
798.890242	45007.343964	33.125248
799.820267	45097.114067	33.130266
800.563170	45148.796065	33.135284
801.391137	45234.258019	33.140301
802.062048	45302.612024	33.145319
803.062706	45375.355696	33.150336
804.239105	45444.314381	33.155354
804.859388	45510.535179	33.160372
805.735677	45572.118963	33.165389
806.606338	45639.773683	33.170407
807.269117	45726.655609	33.175424
808.220832	45793.518787	33.180442
809.284195	45860.058433	33.185460
810.071228	45934.923788	33.190477
810.679948	46001.457465	33.195495
811.484046	46067.733147	33.200512
812.182315	46156.340430	33.205530
812.965655	46220.809091	33.210548
813.948881	46304.077848	33.215565
814.615875	46371.080047	33.220583
815.353707	46442.904595	33.225600
816.038432	46534.812861	33.230618
817.422301	46596.480374	33.235636
818.204842	46677.000167	33.240653
818.425035	46749.337435	33.245671
819.741983	46813.846397	33.250688
820.481811	46888.855857	33.255706
821.289541	46958.355608	33.260724
821.968648	47040.341691	33.265741
822.676625	47109.403590	33.270759
823.729033	47192.731816	33.275776
824.118360	47282.431979	33.280794
825.600254	47346.077396	33.285812
826.281144	47426.632581	33.290829
826.875140	47500.809671	33.295847
828.137281	47572.078970	33.300864
828.702320	47642.077548	33.305882
829.732808	47718.022385	33.310900
830.407784	47789.086273	33.315917
831.396983	47872.146969	33.320935
832.056956	47941.304965	33.325952
832.879715	48016.498504	33.330970
833.886404	48068.159764	33.335988
834.432941	48135.418196	33.341005
834.971404	48201.356117	33.346023
836.058900	48269.892037	33.351040
836.849542	48348.181107	33.356058
837.685246	48408.740074	33.361076
838.115865	48474.162934	33.366093
838.784799	48555.684391	33.371111
840.120766	48624.368308	33.376128
840.505880	48712.527143	33.381146
841.890734	48774.347299	33.386164
842.592777	48858.739414	33.391181
843.198317	48926.644628	33.396199
843.986157	49008.635178	33.401216
844.573586	49099.060867	33.406234
845.565353	49169.161664	33.411252
846.106848	49264.480107	33.416269
846.941703	49346.146036	33.421287
848.155958	49430.494065	33.426304
848.703171	49523.948106	33.431322
849.875999	49608.221531	33.436340
850.927960	49681.489212	33.441357
851.987090	49768.561504	33.446375
852.850972	49843.907728	33.451392
853.478998	49932.062359	33.456410
854.605940	49992.239592	33.461428
855.815853	50088.828754	33.466445
856.605713	50154.323704	33.471463
857.684088	50228.955815	33.476480
858.278885	50312.636647	33.481498
859.104185	50373.771998	33.486516
860.287630	50461.834550	33.491533
860.825062	50532.593673	33.496551
861.805738	50609.218374	33.501568
862.266947	50697.466452	33.506586
863.239408	50764.364116	33.511604
864.109646	50856.091745	33.516621
864.799379	50930.362619	33.521639
865.694629	51015.030856	33.526656
866.576375	51109.074275	33.531674
867.510514	51187.854788	33.536692
868.618925	51267.671418	33.541709
869.373450	51363.405837	33.546727
870.570105	51421.740122	33.551744
871.017090	51516.183073	33.556762
872.087816	51583.484737	33.561780
873.270742	51678.073361	33.566797
873.573081	51755.580956	33.571815
874.886333	51824.110440	33.576832
875.537682	51915.329204	33.581850
876.220132	51996.419270	33.586868
877.484690	52068.488918	33.591885
878.306687	52162.566308	33.596903
879.534744	52238.186585	33.601920
880.088524	52321.299477	33.606938
881.022932	52383.800343	33.611956
881.573871	52460.747521	33.616973
881.996468	52535.487302	33.621991
883.413956	52598.499061	33.627008
883.870578	52680.265665	33.632026
884.733807	52752.629159	33.637044
885.571918	52833.464679	33.642061
886.587518	52925.296529	33.647079
887.206487	52991.072066	33.652096
888.027342	53093.764343	33.657114
888.865075	53166.575412	33.662132
889.890228	53247.057940	33.667149
890.559880	53346.430202	33.672167
891.583220	53435.845798	33.677184
892.558201	53521.475789	33.682202
893.234303	53612.948542	33.687220
894.476558	53694.411659	33.692237
895.303796	53793.057459	33.697255
896.259238	53879.358220	33.702272
897.281791	53959.557115	33.707290
898.112974	54051.638660	33.712308
899.006257	54130.413303	33.717325
899.873597	54218.292065	33.722343
901.027300	54300.838836	33.727360
902.075029	54395.365385	33.732378
902.941632	54480.076563	33.737396
904.080029	54559.959827	33.742413
904.780543	54658.942981	33.747431
905.602062	54735.531667	33.752448
906.288756	54824.635227	33.757466
907.276077	54911.478727	33.762484
908.387531	54991.548093	33.767501
909.160449	55090.629391	33.772519
910.652396	55168.940815	33.777536
911.681873	55261.031655	33.782554
912.426459	55343.256856	33.787572
913.194862	55419.620134	33.792589
914.036056	55505.334431	33.797607
915.008633	55576.378680	33.802624
915.983721	55681.864067	33.807642
916.910891	55761.912479	33.812660
917.652771	55845.819674	33.817677
918.322587	55946.418247	33.822695
919.892344	56013.691726	33.827712
920.524814	56112.308482	33.832730
921.569169	56188.151254	33.837748
922.592459	56273.720226	33.842765
923.177007	56359.861323	33.847783
924.214962	56436.801512	33.852800
925.086119	56545.073676	33.857818
925.981465	56621.639587	33.862836
927.156241	56712.717094	33.867853
927.739144	56799.536059	33.872871
928.765261	56888.302090	33.877888
929.713596	56964.801023	33.882906
930.676452	57052.611937	33.887924
931.853886	57115.677586	33.892941
932.285691	57188.465148	33.897959
933.335404	57264.974455	33.902976
934.183328	57343.789121	33.907994
934.903154	57427.969079	33.913012
935.737550	57522.362643	33.918029
936.424569	57601.371327	33.923047
937.686458	57676.566887	33.928064
938.460059	57778.604842	33.933082
939.254998	57856.337833	33.938100
940.301234	57959.795074	33.943117
941.266426	58034.325829	33.948135
942.288818	58130.760409	33.953152
942.940533	58226.307369	33.958170
943.688366	58315.010900	33.963188
945.080876	58409.528563	33.968205
946.062521	58509.150732	33.973223
947.087482	58610.389279	33.978240
947.755064	58694.273926	33.983258
948.610406	58797.778854	33.988276
949.618987	58881.307011	33.993293
950.468580	58991.693287	33.998311
951.435778	59081.195909	34.003328
952.353422	59198.294153	34.008346
953.631077	59289.945776	34.013364
954.663532	59390.413876	34.018381
955.302954	59499.141189	34.023399
956.625830	59578.458107	34.028416
957.527291	59688.676093	34.033434
958.240859	59788.720335	34.038452
959.520125	59870.621769	34.043469
960.583216	59990.139276	34.048487
962.023665	60077.705435	34.053504
962.699513	60168.933022	34.058522
963.338249	60269.512707	34.063540
964.662583	60356.621891	34.068557
965.369754	60447.299630	34.073575
966.545966	60553.434411	34.078592
967.621053	60644.382941	34.083610
968.185456	60752.750600	34.088628
969.254434	60841.257209	34.093645
970.427933	60942.920533	34.098663
971.611010	61041.194911	34.103680
972.704959	61136.332806	34.108698
973.566823	61237.014806	34.113716
974.465045	61319.636824	34.118733
975.352258	61423.883797	34.123751
976.534352	61514.465883	34.128768
977.569871	61605.652719	34.133786
978.414901	61702.279253	34.138804
979.338282	61796.194066	34.143821
980.174585	61888.787528	34.148839
981.348615	61976.850188	34.153856
982.088794	62083.069311	34.158874
983.206222	62169.923026	34.163892
984.101824	62241.813448	34.168909
984.519830	62337.655447	34.173927
985.644359	62428.592126	34.178944
986.774577	62519.563073	34.183962
987.593221	62614.925922	34.188980
988.593056	62704.791192	34.193997
989.209868	62806.101595	34.199015
990.302162	62900.901320	34.204032
991.229999	62996.842389	34.209050
991.967189	63105.215044	34.214068
993.308097	63188.659024	34.219085
993.957961	63310.890713	34.224103
995.042780	63407.825721	34.229120
996.322498	63513.685998	34.234138
996.896968	63624.294873	34.239156
998.066465	63729.343358	34.244173
998.853832	63837.039572	34.249191
1000.078867	63943.125685	34.254208
1001.096843	64056.262364	34.259226
1002.201713	64167.961635	34.264244
1003.673960	64267.327904	34.269261
1004.725525	64377.135757	34.274279
1005.845872	64466.668086	34.279296
1006.815817	64574.279425	34.284314
1008.098734	64674.246391	34.289332
1009.423150	64764.429804	34.294349
1010.320236	64869.540553	34.299367
1011.422062	64967.466141	34.304384
1012.352653	65068.119688	34.309402
1012.811602	65152.075783	34.314420
1014.074353	65257.389466	34.319437
1015.049179	65363.877009	34.324455
1015.970983	65461.843241	34.329472
1017.285627	65568.195750	34.334490
1018.036166	65671.404539	34.339508
1019.116170	65779.046210	34.344525
1020.050208	65878.888639	34.349543
1021.127590	65981.273323	34.354560
1022.237637	66082.320548	34.359578
1023.004886	66193.586352	34.364596
1024.505097	66290.460457	34.369613
1024.957008	66396.263117	34.374631
1026.303587	66494.495522	34.379648
1027.240491	66610.449057	34.384666
1028.407084	66710.464109	34.389684
1029.517077	66814.780997	34.394701
1030.429543	66933.851425	34.399719
1031.516095	67031.123543	34.404736
1032.629056	67140.861661	34.409754
1033.447861	67242.630905	34.414772
1034.490802	67333.802937	34.419789
1035.597475	67449.406023	34.424807
1036.850686	67547.311208	34.429824
1037.901322	67653.410862	34.434842
1039.254854	67731.446245	34.439860
1039.957526	67818.505357	34.444877
1040.993017	67919.814128	34.449895
1041.979014	67997.978539	34.454912
1043.384472	68089.999840	34.459930
1043.636869	68189.564666	34.464948
1044.649028	68267.012144	34.469965
1045.721373	68373.655581	34.474983
1046.488888	68469.936995	34.480000
1047.624482	68586.951050	34.485018
1048.793491	68675.576048	34.490036
1050.033497	68778.878365	34.495053
1051.088537	68876.625943	34.500071
1051.970860	68965.070431	34.505088
1053.339196	69077.084804	34.510106
1053.985768	69183.212865	34.515124
1055.299055	69281.129879	34.520141
1056.435758	69383.624221	34.525159
1057.136402	69502.924159	34.530176
1058.330561	69604.822973	34.535194
1059.175271	69718.851241	34.540212
1060.269688	69826.819544	34.545229
1060.911637	69951.741806	34.550247
1062.135835	70057.574246	34.555264
1063.389409	70179.418616	34.560282
1064.182338	70296.636419	34.565300
1065.551765	70405.353919	34.570317
1066.542910	70537.142616	34.575335
1067.606108	70640.653489	34.580352
1068.746511	70767.352865	34.585370
1069.623845	70878.988109	34.590388
1070.934260	70989.537869	34.595405
1071.889108	71106.621021	34.600423
1073.123774	71223.925731	34.605440
1074.915374	71327.254862	34.610458
1075.478567	71442.582624	34.615476
1076.821780	71552.928144	34.620493
1078.290940	71663.879775	34.625511
1079.229973	71761.173671	34.630528
1080.518000	71873.690680	34.635546
1081.319506	71984.263777	34.640564
1082.507319	72083.168830	34.645581
1083.254840	72210.104246	34.650599
1084.367106	72304.327691	34.655616
1085.570747	72412.640335	34.660634
1086.701899	72518.418659	34.665652
1087.572695	72653.128277	34.670669
1088.987193	72749.529972	34.675687
1089.725037	72869.577354	34.680704
1090.874516	72979.140194	34.685722
1092.109037	73102.515853	34.690740
1093.175876	73200.232491	34.695757
1094.393837	73314.152666	34.700775
1095.460924	73430.050058	34.705792
1096.624224	73518.135401	34.710810
1097.601641	73630.977176	34.715828
1098.367640	73726.974908	34.720845
1099.844583	73826.525124	34.725863
1100.858401	73927.482836	34.730880
1101.658776	74036.272885	34.735898
1102.431817	74134.609557	34.740916
1103.836302	74242.735922	34.745933
1104.502226	74360.111710	34.750951
1105.276938	74468.914511	34.755968
1106.580910	74576.218194	34.760986
1107.529697	74694.271359	34.766004
1108.438636	74818.979604	34.771021
1109.606523	74939.830478	34.776039
1110.690498	75065.548811	34.781056
1112.078737	75181.139854	34.786074
1112.689753	75316.932510	34.791092
1113.968015	75435.519035	34.796109
1115.402787	75560.337842	34.801127
1116.848573	75688.258649	34.806144
1118.335699	75809.158772	34.811162
1119.299683	75934.591948	34.816180
1120.524080	76052.748289	34.821197
1121.192314	76166.152756	34.826215
1122.683539	76292.041492	34.831232
1123.604239	76404.048365	34.836250
1124.840927	76535.148801	34.841268
1126.141853	76648.619674	34.846285
1127.464704	76765.336201	34.851303
1128.306397	76885.302600	34.856320
1129.437074	77003.523639	34.861338
1130.512164	77124.446595	34.866356
1131.717418	77256.953453	34.871373
1132.618371	77382.923879	34.876391
1134.094208	77505.776249	34.881408
1135.348733	77636.577592	34.886426
1135.694144	77766.051706	34.891444
1137.326836	77890.986136	34.896461
1138.619280	78013.188131	34.901479
1139.587987	78140.365989	34.906496
1140.996624	78263.233615	34.911514
1141.790624	78392.596120	34.916532
1143.091319	78517.195308	34.921549
1144.543686	78639.969759	34.926567
1145.528128	78765.619412	34.931584
1146.646053	78892.904634	34.936602
1147.627124	79021.217407	34.941620
1148.598154	79144.368499	34.946637
1150.085424	79277.994011	34.951655
1151.364802	79407.841970	34.956672
1153.040228	79523.329893	34.961690
1153.797008	79655.462194	34.966708
1154.668394	79775.826419	34.971725
1156.326705	79890.130782	34.976743
1157.461654	80020.195205	34.981760
1158.871838	80131.145959	34.986778
1160.037010	80246.965608	34.991796
1160.981590	80338.674184	34.996813
1162.472505	80447.850205	35.001831
1163.081187	80543.108716	35.006848
1164.484840	80652.312338	35.011866
1165.733974	80759.012597	35.016884
1166.569990	80860.191062	35.021901
1167.672159	80972.718755	35.026919
1168.768197	81085.899135	35.031936
1170.088988	81190.990920	35.036954
1170.815384	81312.480755	35.041972
1172.202381	81421.103188	35.046989
1172.958007	81548.993417	35.052007
1173.832332	81666.972325	35.057024
1175.606260	81787.539782	35.062042
1176.403598	81920.236390	35.067060
1177.475224	82035.303350	35.072077
1178.746850	82176.100085	35.077095
1179.890281	82298.578767	35.082112
1181.330972	82423.021228	35.087130
1182.263535	82557.906693	35.092148
1183.547018	82685.757893	35.097165
1185.166227	82812.311079	35.102183
1186.018291	82949.323382	35.107200
1187.274276	83068.842659	35.112218
1188.448673	83208.795702	35.117236
1189.593345	83340.655847	35.122253
1191.036315	83463.055788	35.127271
1191.989395	83596.636005	35.132288
1193.409466	83730.288228	35.137306
1194.463735	83866.939295	35.142324
1195.836783	83984.124919	35.147341
1197.198687	84112.655154	35.152359
1198.186036	84253.719687	35.157376
1199.527783	84372.657414	35.162394
1200.830704	84502.855868	35.167412
1202.117133	84648.174722	35.172429
1203.351743	84770.665979	35.177447
1204.314567	84901.376184	35.182464
1206.072405	85017.937346	35.187482
1206.747742	85165.829040	35.192500
1208.025234	85288.936095	35.197517
1209.426932	85411.771210	35.202535
1210.631051	85552.759360	35.207552
1211.612372	85684.584252	35.212570
1212.985402	85821.867486	35.217588
1214.183611	85949.612947	35.222605
1215.724620	86076.583865	35.227623
1216.760364	86217.495705	35.232640
1218.051015	86329.478368	35.237658
1219.369142	86471.554674	35.242676
1220.387659	86596.582084	35.247693
1221.671367	86717.907007	35.252711
1222.894156	86856.137639	35.257728
1223.929364	86984.357833	35.262746
1225.228381	87107.269643	35.267764
1226.339364	87209.724843	35.272781
1227.805642	87333.939237	35.277799
1228.664829	87458.775705	35.282816
1230.040092	87560.204132	35.287834
1231.061090	87682.847281	35.292852
1232.108396	87820.663079	35.297869
1233.352066	87934.217168	35.302887
1234.291143	88069.130344	35.307904
1235.791702	88193.477056	35.312922
1237.024633	88330.159993	35.317940
1237.902789	88449.232127	35.322957
1239.125555	88591.457789	35.327975
1240.271773	88738.401359	35.332992
1241.684700	88861.475832	35.338010
1242.781068	89015.979708	35.343028
1243.859917	89153.147661	35.348045
1245.647125	89289.122493	35.353063
1246.449597	89427.132921	35.358080
1247.612611	89573.466077	35.363098
1249.147456	89724.016092	35.368116
1250.176934	89868.064223	35.373133
1251.638512	90019.001046	35.378151
1252.679986	90169.019149	35.383168
1254.393404	90310.027104	35.388186
1255.421165	90447.470642	35.393204
1256.728466	90609.661466	35.398221
1258.258483	90754.717325	35.403239
1259.307416	90900.324949	35.408256
1260.741214	91044.670737	35.413274
1261.856343	91192.660381	35.418292
1263.655715	91329.771774	35.423309
1265.190868	91480.163109	35.428327
1266.373667	91619.056637	35.433344
1267.741709	91753.089652	35.438362
1269.317784	91888.551391	35.443380
1270.115381	92035.433478	35.448397
1271.561628	92162.347693	35.453415
1272.774968	92323.086168	35.458432
1273.611132	92456.094874	35.463450
1275.149088	92592.534692	35.468468
1276.595970	92745.168708	35.473485
1278.192937	92872.031429	35.478503
1278.970045	93017.892363	35.483520
1280.456741	93151.706305	35.488538
1281.811067	93289.444607	35.493556
1283.041652	93439.056512	35.498573
1284.547978	93580.927999	35.503591
1285.861789	93723.223153	35.508608
1287.138997	93856.062636	35.513626
1288.387444	93989.824636	35.518644
1289.335507	94136.525971	35.523661
1290.769589	94276.648652	35.528679
1291.950329	94419.045316	35.533696
1293.378747	94550.479670	35.538714
1294.611575	94679.554901	35.543732
1295.530041	94806.232919	35.548749
1296.886535	94934.138741	35.553767
1298.005989	95067.428002	35.558784
1299.133049	95200.343643	35.563802
1300.604387	95337.386537	35.568820
1301.826327	95473.173168	35.573837
1303.118668	95609.936228	35.578855
1304.280871	95749.674896	35.583872
1305.365949	95894.949036	35.588890
1307.144367	96030.131873	35.593908
1308.136062	96175.903428	35.598925
1309.281334	96324.049005	35.603943
1310.796700	96463.849837	35.608960
1312.248553	96616.402015	35.613978
1313.666618	96765.120742	35.618996
1314.846358	96911.847686	35.624013
1316.014609	97050.018284	35.629031
1317.031393	97207.995436	35.634048
1318.328874	97347.115196	35.639066
1319.865198	97504.202088	35.644084
1321.294054	97658.359141	35.649101
1322.937196	97820.688321	35.654119
1324.258310	97973.586737	35.659136
1325.697058	98120.875007	35.664154
1327.044393	98265.641884	35.669172
1328.312106	98432.703968	35.674189
1329.830369	98565.381108	35.679207
1330.958126	98718.726478	35.684224
1332.166933	98879.208984	35.689242
1333.929160	99022.187571	35.694260
1334.731036	99175.018405	35.699277
1336.483255	99336.929812	35.704295
1338.025140	99487.177708	35.709312
1339.293101	99639.811024	35.714330
1340.388866	99785.462639	35.719348
1341.799732	99953.012878	35.724365
1343.492763	100094.003542	35.729383
1344.725391	100239.003588	35.734400
1346.145390	100392.794542	35.739418
1347.471722	100540.647704	35.744436
1348.620406	100699.665637	35.749453
1350.068118	100843.091496	35.754471
1351.801580	100994.153952	35.759488
1352.873130	101150.681706	35.764506
1354.219358	101299.441342	35.769524
1355.636579	101447.089708	35.774541
1356.992779	101614.818868	35.779559
1358.147989	101771.514676	35.784576
1359.736714	101922.372074	35.789594
1361.176772	102063.364332	35.794612
1362.249175	102236.673239	35.799629
1363.713929	102386.085374	35.804647
1364.954598	102544.588791	35.809664
1366.259903	102689.959603	35.814682
1368.055297	102828.603102	35.819700
1368.978542	102979.845192	35.824717
1370.602264	103098.313365	35.829735
1371.878787	103243.445411	35.834752
1373.172605	103385.911616	35.839770
1374.604786	103508.753157	35.844788
1375.560854	103664.183447	35.849805
1376.776006	103805.215621	35.854823
1378.431870	103953.120328	35.859840
1379.456044	104105.669833	35.864858
1380.810278	104268.741966	35.869876
1382.125626	104417.722514	35.874893
1383.275854	104576.766591	35.879911
1384.700190	104748.190298	35.884928
1385.949831	104908.904091	35.889946
1387.786241	105069.392831	35.894964
1389.111358	105228.445132	35.899981
1390.559319	105403.173175	35.904999
1391.984978	105550.441004	35.910016
1393.440301	105719.019047	35.915034
1394.768409	105877.347449	35.920052
1396.125440	106052.537703	35.925069
1397.593502	106210.554967	35.930087
1399.142447	106388.419468	35.935104
1400.320240	106556.705793	35.940122
1402.149188	106706.543048	35.945140
1403.305301	106880.486584	35.950157
1404.733551	107048.198621	35.955175
1406.206682	107207.360837	35.960192
1407.704251	107375.950179	35.965210
1409.414599	107535.412300	35.970228
1410.436467	107704.864322	35.975245
1411.952131	107875.213726	35.980263
1413.572402	108037.528861	35.985280
1414.853058	108213.614103	35.990298
1416.745904	108373.445169	35.995316
1418.120278	108537.593874	36.000333
1419.356084	108707.417667	36.005351
1421.097872	108873.352052	36.010368
1422.256957	109038.740914	36.015386
1423.789272	109195.229552	36.020404
1425.025372	109364.076849	36.025421
1426.780511	109527.861607	36.030439
1428.084346	109680.186956	36.035456
1429.685738	109851.618958	36.040474
1431.004011	110004.406090	36.045492
1432.555806	110182.937358	36.050509
1433.857644	110335.906401	36.055527
1435.832088	110498.238665	36.060544
1437.125879	110660.977658	36.065562
1438.723292	110813.852081	36.070580
1439.961802	110969.993677	36.075597
1441.272046	111136.974153	36.080615
1442.927865	111297.412755	36.085632
1444.203084	111454.349153	36.090650
1445.722115	111599.803301	36.095668
1447.025019	111735.892656	36.100685
1448.200867	111891.125874	36.105703
1450.007831	112037.574971	36.110720
1451.314325	112183.154948	36.115738
1452.600386	112318.845065	36.120756
1453.754437	112483.036235	36.125773
1455.202675	112625.083052	36.130791
1456.819846	112787.392215	36.135808
1457.928437	112941.876743	36.140826
1459.235834	113094.887331	36.145844
1460.880673	113261.803657	36.150861
1462.202156	113431.298307	36.155879
1463.344675	113598.860109	36.160896
1464.779689	113764.211537	36.165914
1466.326806	113931.907529	36.170932
1467.509429	114109.987706	36.175949
1469.186769	114289.763112	36.180967
1470.825483	114464.304164	36.185984
1472.294563	114641.969093	36.191002
1473.782871	114804.153563	36.196020
1475.203102	114985.899347	36.201037
1476.705979	115173.134801	36.206055
1478.449185	115347.450127	36.211072
1479.960971	115526.823845	36.216090
1481.771682	115692.457471	36.221108
1483.032807	115875.089612	36.226125
1484.376518	116043.484078	36.231143
1486.237224	116226.998473	36.236160
1487.985993	116389.993772	36.241178
1489.428368	116562.598872	36.246196
1490.912889	116732.697615	36.251213
1492.610959	116915.001896	36.256231
1494.224568	117070.450837	36.261248
1495.306849	117249.221173	36.266266
1497.151545	117422.553261	36.271284
1498.387157	117605.062568	36.276301
1499.841497	117773.355913	36.281319
1501.776625	117936.768355	36.286336
1502.888965	118118.420818	36.291354
1504.418976	118294.803627	36.296372
1506.478042	118474.978560	36.301389
1507.802496	118643.830099	36.306407
1509.569714	118810.313981	36.311424
1511.181479	118992.437788	36.316442
1512.605062	119145.612052	36.321460
1514.075833	119325.202550	36.326477
1515.410327	119495.077482	36.331495
1517.137232	119660.230877	36.336512
1518.097714	119831.180538	36.341530
1519.687091	119996.592204	36.346548
1521.347731	120182.933733	36.351565
1522.800680	120351.275745	36.356583
1524.240345	120514.985823	36.361600
1525.577459	120702.129652	36.366618
1527.392806	120871.671221	36.371636
1528.551114	121028.033164	36.376653
1529.896413	121189.216882	36.381671
1531.428923	121348.700110	36.386688
1532.750125	121514.220978	36.391706
1534.244342	121679.728068	36.396724
1536.010394	121852.893295	36.401741
1537.349919	122016.134722	36.406759
1539.053574	122190.958536	36.411776
1540.375660	122371.378809	36.416794
1541.906773	122535.036291	36.421812
1543.355997	122716.211300	36.426829
1544.920440	122893.873585	36.431847
1546.700861	123072.148692	36.436864
1548.003207	123254.718588	36.441882
1549.413805	123439.375046	36.446900
1551.028094	123627.154207	36.451917
1552.191639	123825.506302	36.456935
1553.838575	123993.004792	36.461952
1555.062015	124206.004711	36.466970
1556.965193	124393.110064	36.471988
1558.476306	124589.867344	36.477005
1559.976890	124780.915225	36.482023
1561.791094	124985.189055	36.487040
1563.683334	125182.827452	36.492058
1565.381435	125365.386878	36.497076
1566.841045	125559.144778	36.502093
1568.515761	125749.310534	36.507111
1570.408760	125948.436433	36.512128
1571.635177	126135.496729	36.517146
1573.656586	126319.885956	36.522164
1575.312197	126509.388730	36.527181
1576.337067	126703.755892	36.532199
1578.171204	126906.711008	36.537216
1579.583787	127091.379519	36.542234
1581.643118	127281.735594	36.547252
1583.139446	127479.048255	36.552269
1584.695963	127679.418356	36.557287
1586.585743	127854.667480	36.562304
1587.820651	128061.970056	36.567322
1590.048361	128236.699234	36.572340
1591.752630	128425.966877	36.577357
1593.050662	128614.578264	36.582375
1594.914196	128797.552450	36.587392
1596.333999	128981.497778	36.592410
1597.803266	129172.974148	36.597428
1599.520292	129361.676104	36.602445
1601.299230	129553.942040	36.607463
1602.850873	129728.572683	36.612480
1604.159693	129928.922453	36.617498
1605.970488	130115.182246	36.622516
1607.856848	130303.546985	36.627533
1609.004374	130489.825948	36.632551
1611.024195	130678.172019	36.637568
1612.268152	130851.072230	36.642586
1614.029430	131031.936288	36.647604
1615.335880	131198.861522	36.652621
1616.959193	131371.818715	36.657639
1618.804055	131539.610663	36.662656
1620.319254	131712.751828	36.667674
1621.824519	131871.832392	36.672692
1623.808912	132046.586144	36.677709
1624.913337	132217.793845	36.682727
1626.432684	132393.447137	36.687744
1627.985843	132583.628525	36.692762
1629.013293	132771.690106	36.697780
1630.944408	132952.311449	36.702797
1632.229303	133145.972798	36.707815
1633.940162	133336.691669	36.712832
1635.183049	133545.059883	36.717850
1636.925064	133738.247205	36.722868
1639.256563	133938.133602	36.727885
1640.580968	134139.042943	36.732903
1642.342269	134345.915549	36.737920
1644.062094	134538.769688	36.742938
1645.714285	134738.009303	36.747956
1647.144857	134928.251112	36.752973
1648.805505	135145.130154	36.757991
1650.734269	135341.567732	36.763008
1652.354720	135547.482989	36.768026
1654.211969	135759.330288	36.773044
1655.867211	135955.397317	36.778061
1657.541056	136164.869140	36.783079
1659.341839	136357.570498	36.788096
1661.113696	136563.126780	36.793114
1662.531413	136760.098625	36.798132
1664.525350	136954.876766	36.803149
1666.170924	137167.046702	36.808167
1668.177528	137360.710405	36.813184
1669.631629	137558.505523	36.818202
1671.445053	137772.642700	36.823220
1673.487230	137964.023742	36.828237
1674.834392	138164.526434	36.833255
1676.498354	138358.973447	36.838272
1678.097195	138573.961555	36.843290
1680.015439	138761.603712	36.848308
1681.876195	138971.876927	36.853325
1683.258401	139175.257598	36.858343
1684.790050	139362.534071	36.863360
1686.658258	139583.341572	36.868378
1688.568341	139771.143474	36.873396
1690.460181	139962.434561	36.878413
1691.974922	140171.744669	36.883431
1693.724866	140362.832731	36.888448
1695.475191	140569.510185	36.893466
1697.118058	140759.122316	36.898484
1698.835505	140961.093162	36.903501
1700.372197	141165.223232	36.908519
1702.181285	141346.295996	36.913536
1704.001995	141562.537724	36.918554
1705.503906	141739.428577	36.923572
1707.391190	141906.373606	36.928589
1708.482108	142101.088004	36.933607
1710.086853	142278.612045	36.938624
1711.786936	142459.391916	36.943642
1713.348588	142658.838639	36.948660
1715.054230	142841.812538	36.953677
1716.381813	143042.287528	36.958695
1718.253700	143243.361825	36.963712
1719.878556	143434.666556	36.968730
1721.451631	143641.785978	36.973748
1723.685385	143843.871420	36.978765
1724.932785	144044.353008	36.983783
1726.758492	144253.540449	36.988800
1728.545854	144464.395817	36.993818
1730.294996	144674.865763	36.998836
1732.032255	144877.936738	37.003853
1733.569280	145092.752751	37.008871
1735.026453	145310.054614	37.013888
1736.792223	145517.194015	37.018906
1738.484868	145740.837224	37.023924
1740.782259	145957.439790	37.028941
1742.325527	146190.895489	37.033959
1744.071870	146395.977658	37.038976
1745.972474	146616.868811	37.043994
1747.580514	146841.661453	37.049012
1749.583496	147051.511331	37.054029
1751.171434	147291.318788	37.059047
1753.088180	147497.851502	37.064064
1755.179976	147729.685005	37.069082
1756.733605	147945.861573	37.074100
1759.006875	148167.249471	37.079117
1760.853807	148384.776864	37.084135
1762.744326	148592.791338	37.089152
1764.673842	148813.148107	37.094170
1766.296329	149018.292255	37.099188
1767.814452	149227.029169	37.104205
1769.588702	149449.975696	37.109223
1771.594075	149670.402368	37.114240
1773.126585	149885.378384	37.119258
1774.810776	150097.149763	37.124276
1777.203012	150309.507369	37.129293
1778.822544	150527.453005	37.134311
1780.754072	150741.420550	37.139328
1782.601525	150953.070179	37.144346
1784.235585	151174.567564	37.149364
1786.318767	151373.073806	37.154381
1787.802957	151589.526706	37.159399
1789.710552	151806.446290	37.164416
1791.953664	152009.875386	37.169434
1793.153240	152231.131945	37.174452
1795.392567	152431.077783	37.179469
1796.960916	152640.018786	37.184487
1798.676493	152862.478162	37.189504
1800.587884	153070.175664	37.194522
1801.989037	153265.555937	37.199540
1804.030668	153447.371085	37.204557
1805.486661	153647.271131	37.209575
1807.291442	153851.491150	37.214592
1809.202954	154033.748555	37.219610
1810.576711	154244.708428	37.224628
1812.736530	154433.331404	37.229645
1813.830947	154643.475967	37.234663
1815.906123	154838.720409	37.239680
1817.576225	155062.177962	37.244698
1818.828737	155271.312374	37.249716
1821.177580	155479.906345	37.254733
1822.914188	155711.383631	37.259751
1824.312414	155924.011135	37.264768
1826.730738	156148.586998	37.269786
1828.467396	156357.752697	37.274804
1830.602705	156576.531009	37.279821
1832.025534	156801.700316	37.284839
1833.830646	157023.399538	37.289856
1836.024598	157249.730051	37.294874
1837.748302	157481.208718	37.299892
1839.855530	157696.194631	37.304909
1841.586331	157926.939723	37.309927
1843.277599	158151.783619	37.314944
1845.582109	158370.483101	37.319962
1847.403903	158605.719805	37.324980
1849.566698	158821.236474	37.329997
1851.389446	159052.012502	37.335015
1853.060371	159277.450225	37.340032
1855.006825	159507.841892	37.345050
1856.870966	159722.612647	37.350068
1859.054539	159946.033135	37.355085
1860.808179	160182.343793	37.360103
1862.709090	160399.306666	37.365120
1864.637009	160617.636154	37.370138
1866.288584	160857.759209	37.375156
1868.232441	161071.282770	37.380173
1870.406791	161309.601247	37.385191
1872.211617	161519.548049	37.390208
1874.216638	161746.774661	37.395226
1876.186617	161965.016988	37.400244
1878.003626	162183.348337	37.405261
1879.973269	162413.374782	37.410279
1881.535112	162643.771793	37.415296
1883.919713	162857.756040	37.420314
1885.329473	163094.368872	37.425332
1887.535538	163311.186880	37.430349
1889.604444	163540.164829	37.435367
1891.529884	163756.674944	37.440384
1893.666694	163978.555487	37.445402
1895.322512	164193.589113	37.450420
1897.367062	164406.850171	37.455437
1899.523783	164619.841020	37.460455
1900.878266	164847.900604	37.465472
1903.139244	165049.044481	37.470490
1905.097343	165251.188740	37.475508
1906.988732	165449.438373	37.480525
1908.479535	165640.726304	37.485543
1910.476323	165827.876360	37.490560
1912.419676	166022.087628	37.495578
1913.940394	166229.050120	37.500596
1915.626046	166418.560869	37.505613
1917.262051	166644.798527	37.510631
1919.053430	166842.602200	37.515648
1920.977491	167061.275444	37.520666
1922.629765	167282.238077	37.525684
1924.409582	167499.541585	37.530701
1926.546751	167727.951240	37.535719
1928.281715	167960.472217	37.540736
1930.513797	168175.691140	37.545754
1932.230212	168410.919478	37.550772
1934.240032	168626.759696	37.555789
1936.064363	168873.833263	37.560807
1937.863744	169107.162824	37.565824
1939.979268	169345.098733	37.570842
1941.833833	169578.815624	37.575860
1943.900567	169819.920607	37.580877
1946.071531	170060.414394	37.585895
1947.952763	170296.135554	37.590912
1949.925797	170543.855874	37.595930
1951.878890	170787.648702	37.600948
1954.221861	171009.550772	37.605965
1956.111104	171261.918901	37.610983
1958.011678	171499.026945	37.616000
1960.561881	171734.105227	37.621018
1962.059753	171975.973504	37.626036
1964.517865	172187.830138	37.631053
1966.565330	172433.216588	37.636071
1968.403453	172671.939965	37.641088
1970.659428	172900.539006	37.646106
1972.272559	173142.040955	37.651124
1974.747963	173373.386011	37.656141
1976.976596	173603.173190	37.661159
1978.662984	173841.991111	37.666176
1980.734159	174064.245294	37.671194
1982.605351	174292.976818	37.676212
1985.125087	174531.450958	37.681229
1986.872059	174777.508459	37.686247
1988.735821	175008.313036	37.691264
1990.981215	175234.846598	37.696282
1993.038948	175468.452016	37.701300
1995.425427	175700.839482	37.706317
1997.714560	175911.030033	37.711335
1999.597203	176145.187256	37.716352
2001.408664	176339.242644	37.721370
2003.731643	176575.425720	37.726388
2006.092184	176775.904224	37.731405
2007.751772	176990.640501	37.736423
2009.347010	177205.273926	37.741440
2011.785743	177414.928293	37.746458
2013.224061	177621.126714	37.751476
2015.343865	177805.396613	37.756493
2017.339701	178006.522550	37.761511
2018.787206	178213.826213	37.766528
2020.991242	178398.732412	37.771546
2022.588164	178614.184812	37.776564
2024.590312	178815.250205	37.781581
2026.463840	179033.984913	37.786599
2028.233907	179258.383022	37.791616
2030.372272	179464.669762	37.796634
2032.223809	179686.380184	37.801652
2034.213751	179918.613118	37.806669
2036.061765	180137.662080	37.811687
2038.147531	180368.486634	37.816704
2040.535654	180604.035044	37.821722
2042.524637	180835.435734	37.826740
2044.381440	181068.102051	37.831757
2046.575222	181300.322838	37.836775
2048.556482	181536.727562	37.841792
2050.493694	181767.760834	37.846810
2052.496156	182016.928994	37.851828
2054.544448	182250.205696	37.856845
2056.944569	182491.066161	37.861863
2059.166771	182734.684172	37.866880
2061.495279	182965.357196	37.871898
2063.648922	183207.834069	37.876916
2065.767829	183451.358248	37.881933
2067.818284	183677.955346	37.886951
2069.997756	183921.903922	37.891968
2072.221213	184142.816806	37.896986
2073.979531	184384.144723	37.902004
2076.165295	184631.788635	37.907021
2078.866996	184854.989310	37.912039
2080.352957	185092.240350	37.917056
2082.644291	185322.588916	37.922074
2085.111188	185561.399838	37.927092
2087.118891	185797.252151	37.932109
2089.305002	186037.873931	37.937127
2091.269697	186263.698283	37.942144
2093.669719	186492.703181	37.947162
2095.739904	186724.324823	37.952180
2097.988069	186965.119306	37.957197
2100.732985	187184.530438	37.962215
2102.453096	187412.175797	37.967232
2104.622818	187633.850244	37.972250
2107.095512	187862.660102	37.977268
2109.045624	188073.039526	37.982285
2111.205053	188296.787219	37.987303
2113.182575	188520.501392	37.992320
2115.937932	188740.768470	37.997338
2117.725005	188959.388190	38.002356
2120.044109	189174.828144	38.007373
2122.464511	189390.582962	38.012391
2124.249156	189602.442187	38.017408
2126.092500	189813.785438	38.022426
2128.233622	190003.470732	38.027444
2130.461622	190195.401894	38.032461
2132.691854	190371.559253	38.037479
2134.101781	190573.126842	38.042496
2136.383836	190759.252144	38.047514
2138.098762	190953.171317	38.052532
2140.032148	191166.587534	38.057549
2142.164585	191367.295107	38.062567
2144.017605	191581.182771	38.067584
2146.487255	191788.996199	38.072602
2148.596627	191999.913472	38.077620
2150.665268	192210.965029	38.082637
2152.815993	192421.585678	38.087655
2154.627634	192652.338238	38.092672
2157.013581	192863.393048	38.097690
2159.447843	193094.074313	38.102708
2161.685936	193304.532600	38.107725
2164.026627	193533.301696	38.112743
2166.121815	193751.208941	38.117760
2168.549428	193970.435085	38.122778
2170.457698	194193.348931	38.127796
2172.911372	194406.214450	38.132813
2175.301561	194624.434083	38.137831
2177.234551	194849.897930	38.142848
2179.476260	195065.934689	38.147866
2181.658706	195283.403243	38.152884
2183.512536	195521.853570	38.157901
2186.191836	195739.461040	38.162919
2188.319736	195966.269659	38.167936
2190.707346	196191.946590	38.172954
2192.904752	196416.309330	38.177972
2195.346478	196641.078524	38.182989
2197.786389	196858.703336	38.188007
2199.438515	197092.369961	38.193024
2202.195679	197295.883393	38.198042
2204.162267	197516.530626	38.203060
2206.367852	197746.913971	38.208077
2208.852748	197957.733175	38.213095
2210.723626	198196.497773	38.218112
2213.010539	198410.332913	38.223130
2215.473320	198639.283216	38.228148
2217.314353	198862.380291	38.233165
2219.768010	199089.709339	38.238183
2221.892621	199315.504955	38.243200
2224.156490	199530.922165	38.248218
2226.605460	199774.895065	38.253236
2228.862630	199988.753965	38.258253
2231.405743	200215.426279	38.263271
2233.512322	200435.822294	38.268288
2235.774357	200653.706726	38.273306
2238.173754	200884.047525	38.278324
2240.179201	201106.467803	38.283341
2242.739205	201304.772898	38.288359
2244.610140	201540.480620	38.293376
2246.961238	201740.838641	38.298394
2249.267895	201944.428538	38.303412
2250.954684	202135.957251	38.308429
2253.366969	202322.903511	38.313447
2255.311873	202529.637418	38.318464
2257.686382	202725.971475	38.323482
2259.654354	202924.642829	38.328500
2261.363895	203136.112907	38.333517
2263.714962	203346.326936	38.338535
2265.594283	203564.816664	38.343552
2267.701462	203793.261063	38.348570
2270.263725	203999.559757	38.353588
2272.247857	204251.927881	38.358605
2274.520954	204480.259875	38.363623
2276.888224	204705.544000	38.368640
2279.149430	204938.309885	38.373658
2281.272951	205170.374981	38.378676
2283.392028	205418.575887	38.383693
2285.958550	205650.052208	38.388711
2287.856515	205897.503182	38.393728
2290.134906	206152.511427	38.398746
2292.609041	206397.042342	38.403764
2294.683060	206648.365717	38.408781
2297.266193	206899.888716	38.413799
2299.724888	207154.936182	38.418816
2302.267629	207399.257254	38.423834
2304.698866	207655.542584	38.428852
2306.909562	207900.768886	38.433869
2309.616528	208147.656674	38.438887
2312.003027	208390.914815	38.443904
2314.549557	208652.302077	38.448922
2317.124274	208882.279010	38.453940
2319.411941	209125.898522	38.458957
2322.035480	209362.458160	38.463975
2324.670937	209605.351606	38.468992
2326.832652	209838.672908	38.474010
2329.109375	210077.321475	38.479028
2331.597801	210317.549676	38.484045
2334.253980	210553.029607	38.489063
2336.331528	210798.796412	38.494080
2338.426364	211036.499949	38.499098
2340.917872	211269.215717	38.504116
2343.073904	211513.436732	38.509133
2345.684821	211758.005519	38.514151
2347.848897	211998.266154	38.519168
2350.369238	212234.954559	38.524186
2352.664668	212473.951994	38.529204
2354.686777	212723.124724	38.534221
2357.327700	212961.243976	38.539239
2359.561294	213211.197574	38.544256
2361.806560	213461.607325	38.549274
2364.602311	213701.050482	38.554292
2366.634143	213945.757422	38.559309
2368.825492	214203.224726	38.564327
2371.392730	214449.295982	38.569344
2373.786971	214683.194747	38.574362
2376.005739	214906.165491	38.579380
2377.996675	215134.543522	38.584397
2380.317046	215334.011890	38.589415
2382.345674	215578.344434	38.594432
2384.441726	215809.120346	38.599450
2386.858180	216034.678889	38.604468
2388.721868	216277.757768	38.609485
2391.436187	216528.587076	38.614503
2393.578878	216769.376218	38.619520
2395.704137	217029.772202	38.624538
2398.183438	217279.549595	38.629556
2400.157485	217537.787656	38.634573
2402.822624	217793.022309	38.639591
2404.891172	218062.864651	38.644608
2407.433964	218326.487678	38.649626
2409.876765	218601.351398	38.654644
2412.058404	218880.904576	38.659661
2414.775270	219151.702102	38.664679
2417.042607	219441.261630	38.669696
2419.583854	219712.584268	38.674714
2421.965206	219985.469588	38.679732
2424.144527	220286.943444	38.684749
2427.257410	220567.561708	38.689767
2429.501338	220842.401932	38.694784
2432.104218	221128.016920	38.699802
2434.751303	221404.128511	38.704820
2437.228071	221698.196578	38.709837
2439.612609	221986.096838	38.714855
2441.765425	222273.298472	38.719872
2444.401280	222568.601724	38.724890
2446.975028	222857.643435	38.729908
2449.481302	223140.437075	38.734925
2452.012852	223429.932020	38.739943
2454.783029	223754.765594	38.744960
2457.041213	224068.025255	38.749978
2459.662889	224352.849292	38.754996
2462.004047	224654.086140	38.760013
2464.630057	224936.867246	38.765031
2467.093557	225224.474867	38.770048
2469.869276	225511.462624	38.775066
2472.653403	225803.897451	38.780084
2475.024879	226093.262335	38.785101
2477.502466	226372.313369	38.790119
2480.222127	226659.085461	38.795136
2482.575132	226944.824617	38.800154
2485.027381	227222.549219	38.805172
2487.594548	227517.195838	38.810189
2490.576591	227793.060616	38.815207
2492.907720	228071.670672	38.820224
2495.025832	228358.543863	38.825242
2497.639209	228638.406247	38.830260
2500.117096	228921.414797	38.835277
2502.552188	229205.675487	38.840295
2505.245828	229493.985018	38.845312
2507.322707	229774.367797	38.850330
2509.909513	230031.203814	38.855348
2512.254615	230292.929714	38.860365
2514.811127	230544.006864	38.865383
2517.155117	230806.928098	38.870400
2519.319648	231070.284885	38.875418
2521.885148	231330.429617	38.880436
2523.480471	231609.243557	38.885453
2525.905164	231884.345858	38.890471
2528.503399	232168.132845	38.895488
2530.907398	232465.996383	38.900506
2533.347103	232754.153259	38.905524
2535.756595	233056.944944	38.910541
2538.496020	233354.986691	38.915559
2541.042774	233663.473065	38.920576
2543.630189	233966.620378	38.925594
2546.215375	234268.854650	38.930612
2548.504723	234580.483271	38.935629
2551.103210	234881.447392	38.940647
2554.053017	235190.281045	38.945664
2556.164452	235505.699692	38.950682
2558.749488	235819.164782	38.955700
2561.733426	236134.624911	38.960717
2564.414114	236448.203754	38.965735
2566.756012	236771.260162	38.970752
2569.385306	237094.805402	38.975770
2572.240734	237406.149716	38.980788
2574.953504	237725.162639	38.985805
2577.261269	238042.157953	38.990823
2580.085701	238363.263188	38.995840
2582.306440	238688.605086	39.000858
2585.105829	239016.599383	39.005876
2587.892686	239348.685928	39.010893
2590.549963	239672.970954	39.015911
2593.464495	240001.661063	39.020928
2595.941887	240318.864562	39.025946
2599.050705	240647.551133	39.030964
2601.343783	240975.605878	39.035981
2603.900355	241293.002675	39.040999
2606.537994	241615.696046	39.046016
2608.864446	241950.860151	39.051034
2611.863336	242264.811248	39.056052
2614.140455	242598.664150	39.061069
2617.366579	242920.200939	39.066087
2619.757592	243253.427950	39.071104
2621.982838	243599.255234	39.076122
2625.126813	243910.622056	39.081140
2627.710214	244245.573802	39.086157
2630.394547	244577.614767	39.091175
2633.160860	244901.109007	39.096192
2635.252689	245233.905896	39.101210
2638.323590	245561.519177	39.106228
2640.859164	245894.374396	39.111245
2643.717654	246217.882585	39.116263
2646.256957	246548.376517	39.121280
2648.619612	246871.050336	39.126298
2651.428631	247171.682367	39.131316
2653.562865	247481.312268	39.136333
2655.934672	247781.583011	39.141351
2658.814122	248086.346148	39.146368
2661.182303	248407.879455	39.151386
2663.735416	248707.361316	39.156404
2666.287399	249018.630124	39.161421
2668.723999	249336.699988	39.166439
2671.451425	249663.513302	39.171456
2673.906275	249994.079077	39.176474
2676.826933	250314.512772	39.181492
2679.371185	250651.644716	39.186509
2681.704873	250988.531289	39.191527
2684.770607	251323.168853	39.196544
2687.506247	251664.311393	39.201562
2690.070614	252000.045776	39.206580
2692.689439	252356.474620	39.211597
2695.534690	252694.934641	39.216615
2698.058655	253043.378322	39.221632
2700.340161	253392.978760	39.226650
2703.194200	253747.137733	39.231668
2705.686517	254119.390094	39.236685
2708.374048	254483.483605	39.241703
2711.694326	254848.493662	39.246720
2714.222994	255214.061616	39.251738
2717.174605	255575.270275	39.256756
2720.258110	255944.917628	39.261773
2722.772184	256306.603304	39.266791
2725.570668	256672.562946	39.271808
2728.334319	257043.253564	39.276826
2731.246898	257411.584196	39.281844
2733.988506	257770.848432	39.286861
2736.739821	258153.634398	39.291879
2739.737130	258513.926192	39.296896
2742.548297	258888.752874	39.301914
2745.507436	259246.435338	39.306932
2748.054618	259631.262774	39.311949
2750.908975	259991.579357	39.316967
2753.844127	260352.137667	39.321984
2756.644790	260723.971177	39.327002
2759.410396	261089.612463	39.332020
2762.385679	261452.198080	39.337037
2764.896885	261825.145799	39.342055
2767.675244	262186.747397	39.347072
2770.448799	262557.596841	39.352090
2773.331757	262928.505605	39.357108
2776.104442	263296.485515	39.362125
2778.846870	263662.870233	39.367143
2781.800606	264034.404094	39.372160
2784.208893	264417.532301	39.377178
2787.391766	264784.204070	39.382196
2789.799205	265158.772338	39.387213
2792.695906	265538.928377	39.392231
2795.869227	265906.009156	39.397248
2798.685127	266266.186388	39.402266
2801.189661	266617.826947	39.407284
2803.843675	266948.232435	39.412301
2806.422655	267291.072207	39.417319
2809.126244	267616.592884	39.422336
2811.565491	267970.505648	39.427354
2814.258424	268317.341770	39.432372
2816.964369	268672.076463	39.437389
2819.410806	269025.963345	39.442407
2822.235781	269385.074374	39.447424
2825.101788	269767.194508	39.452442
2827.784933	270139.309487	39.457460
2830.458264	270510.740312	39.462477
2833.060847	270894.350717	39.467495
2836.019448	271277.955722	39.472512
2838.704216	271673.620037	39.477530
2841.531999	272051.657308	39.482548
2844.514990	272444.912162	39.487565
2847.036649	272848.960412	39.492583
2849.899284	273253.945513	39.497600
2852.995821	273653.177903	39.502618
2855.955358	274044.836436	39.507636
2858.970211	274459.171520	39.512653
2861.438309	274864.092337	39.517671
2864.707927	275266.854001	39.522688
2867.268585	275682.531249	39.527706
2870.609107	276095.747900	39.532724
2874.072741	276505.312348	39.537741
2876.584228	276918.177529	39.542759
2879.689610	277325.029627	39.547776
2882.646451	277749.890781	39.552794
2885.457652	278159.558258	39.557812
2888.780187	278563.200279	39.562829
2891.508092	278979.104540	39.567847
2894.511956	279396.362149	39.572864
2897.208554	279810.442013	39.577882
2900.284908	280226.366824	39.582900
2903.701687	280634.286298	39.587917
2906.425496	281044.372940	39.592935
2909.659656	281450.034593	39.597952
2912.259758	281858.692361	39.602970
2915.193366	282262.953112	39.607988
2918.254243	282673.569662	39.613005
2921.329275	283091.652228	39.618023
2924.810739	283496.333440	39.623040
2927.341403	283911.757982	39.628058
2930.286637	284319.597200	39.633076
2933.438849	284732.636344	39.638093
2936.180469	285148.026381	39.643111
2939.272136	285545.324395	39.648128
2942.058552	285959.410971	39.653146
2944.934909	286363.804308	39.658164
2948.327708	286770.427134	39.663181
2950.648905	287179.581613	39.668199
2953.999733	287576.760250	39.673216
2956.811299	287985.175670	39.678234
2960.009460	288357.152432	39.683252
2962.795052	288731.226296	39.688269
2965.309229	289100.160489	39.693287
2968.256717	289482.133490	39.698304
2970.546454	289861.237981	39.703322
2973.970101	290247.834109	39.708340
2976.717368	290629.710247	39.713357
2979.083512	291025.439818	39.718375
2981.960670	291409.859947	39.723392
2984.640594	291820.754811	39.728410
2987.720725	292233.567054	39.733428
2990.671444	292638.371891	39.738445
2993.409147	293063.480916	39.743463
2996.274012	293481.430960	39.748480
2999.235556	293911.481858	39.753498
3002.382727	294349.174038	39.758516
3005.646173	294771.808794	39.763533
3008.265446	295212.097587	39.768551
3011.368381	295646.364789	39.773568
3014.031095	296101.835277	39.778586
3017.057899	296542.031274	39.783604
3020.306197	296992.580624	39.788621
3023.544502	297452.757812	39.793639
3026.698999	297913.480564	39.798656
3029.691494	298375.421673	39.803674
3032.648422	298813.667411	39.808692
3035.938827	299268.700572	39.813709
3038.638510	299737.263454	39.818727
3042.528040	300185.848947	39.823744
3045.510412	300649.919262	39.828762
3048.321634	301102.076690	39.833780
3051.544588	301552.770605	39.838797
3054.609177	302021.065932	39.843815
3057.832854	302477.802537	39.848832
3061.001402	302943.614668	39.853850
3064.289691	303408.618961	39.858868
3067.530296	303869.539774	39.863885
3070.033218	304332.049096	39.868903
3073.218816	304787.539872	39.873920
3076.297693	305254.425541	39.878938
3079.447262	305729.020205	39.883956
3083.100106	306194.617993	39.888973
3085.990383	306664.932291	39.893991
3089.398404	307119.389386	39.899008
3092.634155	307586.140441	39.904026
3095.605156	308047.318252	39.909044
3098.919897	308504.960170	39.914061
3101.579900	308975.556359	39.919079
3104.718809	309438.429603	39.924096
3108.290924	309901.435714	39.929114
3111.329926	310364.219578	39.934132
3114.451511	310826.124961	39.939149
3117.575272	311286.732781	39.944167
3120.799043	311742.014458	39.949184
3123.833169	312193.209627	39.954202
3126.762647	312616.226502	39.959220
3129.990439	313032.540005	39.964237
3132.334741	313460.167229	39.969255
3135.523471	313878.820353	39.974272
3138.725656	314309.813478	39.979290
3141.428525	314747.487477	39.984308
3144.655515	315190.664378	39.989325
3147.671787	315627.142132	39.994343
3150.315963	316072.515488	39.999360
3153.381097	316534.252882	40.004378
3156.416528	316992.818074	40.009396
3159.475871	317444.113536	40.014413
3162.322242	317914.031796	40.019431
3165.565615	318389.015280	40.024448
3168.939708	318874.922054	40.029466
3171.747771	319360.560306	40.034484
3174.840799	319849.198611	40.039501
3178.278542	320341.284589	40.044519
3181.594216	320824.015719	40.049536
3184.321907	321319.586512	40.054554
3187.638355	321821.461377	40.059572
3190.733879	322315.698563	40.064589
3193.820477	322832.359410	40.069607
3197.011766	323342.956281	40.074624
3200.595485	323863.214728	40.079642
3203.710235	324377.118974	40.084660
3207.093881	324889.631538	40.089677
3210.309830	325407.297371	40.094695
3213.973852	325925.041414	40.099712
3217.098501	326452.060575	40.104730
3220.453082	326970.888046	40.109748
3223.948207	327485.220368	40.114765
3226.831569	328010.515075	40.119783
3229.951027	328525.814177	40.124800
3233.319983	329048.485547	40.129818
3236.499710	329580.020479	40.134836
3239.849909	330109.416985	40.139853
3243.203213	330648.052640	40.144871
3246.692637	331163.199008	40.149888
3250.295519	331697.368989	40.154906
3253.557413	332216.149792	40.159924
3257.305147	332738.252693	40.164941
3260.154296	333264.480604	40.169959
3263.597111	333779.412450	40.174976
3267.054678	334302.260676	40.179994
3270.480932	334830.645465	40.185012
3274.048865	335351.640028	40.190029
3277.001754	335865.643502	40.195047
3280.344419	336381.739722	40.200064
3283.275639	336899.928373	40.205082
3286.608496	337432.395632	40.210100
3290.258055	337939.010971	40.215117
3293.586973	338465.173428	40.220135
3296.586142	338988.235297	40.225152
3300.092248	339486.634574	40.230170
3303.208707	339972.853376	40.235188
3306.878878	340454.613738	40.240205
3309.520732	340936.913887	40.245223
3312.584113	341403.452689	40.250240
3315.900681	341890.208898	40.255258
3318.763862	342377.769245	40.260276
3322.313118	342867.603780	40.265293
3325.153685	343365.163147	40.270311
3328.042125	343868.778755	40.275328
3331.363815	344372.880140	40.280346
3334.501511	344895.920696	40.285364
3337.964916	345419.793670	40.290381
3340.944779	345946.734183	40.295399
3344.519977	346467.914285	40.300416
3347.610095	347003.256422	40.305434
3350.403241	347549.683944	40.310452
3353.864192	348091.760952	40.315469
3357.381900	348644.079995	40.320487
3360.738079	349208.274595	40.325504
3364.215399	349766.808537	40.330522
3367.714650	350329.318922	40.335540
3371.339456	350890.178954	40.340557
3374.401097	351467.800451	40.345575
3377.913626	352026.330940	40.350592
3381.670660	352589.563882	40.355610
3384.703533	353174.101489	40.360628
3388.360287	353736.931857	40.365645
3392.170903	354303.006356	40.370663
3395.691360	354864.729140	40.375680
3399.124254	355439.278293	40.380698
3402.227388	356017.909040	40.385716
3405.833669	356585.107443	40.390733
3409.561118	357168.042901	40.395751
3412.949895	357741.532098	40.400768
3416.779758	358319.158332	40.405786
3420.065718	358889.756889	40.410804
3423.561554	359460.442502	40.415821
3427.161929	360036.891774	40.420839
3430.421356	360611.662157	40.425856
3434.212398	361187.331424	40.430874
3437.796419	361758.229584	40.435892
3441.595341	362326.066651	40.440909
3444.765218	362908.259640	40.445927
3448.213912	363477.889278	40.450944
3451.611229	364037.520706	40.455962
3454.976589	364617.427937	40.460980
3458.740001	365194.600150	40.465997
3462.202240	365767.549128	40.471015
3465.561644	366344.973562	40.476032
3469.057890	366925.769489	40.481050
3472.368503	367491.284829	40.486068
3476.155793	368060.727106	40.491085
3479.514626	368647.130417	40.496103
3482.930350	369222.909680	40.501120
3486.281193	369777.927870	40.506125
3489.341225	370303.196836	40.511130
3492.495361	370786.214081	40.516135
3495.590325	371214.666950	40.521140
3497.968918	371592.833046	40.526144
3500.474446	371921.190933	40.531149
3502.848384	372206.956477	40.536154
3504.918264	372425.888966	40.541159
3506.330830	372629.101219	40.546164
3507.993010	372780.021715	40.551168
3509.592283	372882.567116	40.556173
3510.362338	372971.353815	40.561178
3511.556052	373020.236404	40.566183
3512.652547	373054.430763	40.571188
3513.142838	373063.460348	40.576192
3514.275435	373039.190953	40.581197
3514.471963	372997.847525	40.586202
3515.120616	372939.668468	40.591207
3515.360237	372875.270615	40.596212
3515.728288	372783.963536	40.601216
3516.228887	372690.396685	40.606221
3515.650886	372582.627126	40.611226
3515.836171	372459.982005	40.616231
3516.193383	372346.645495	40.621236
3515.943085	372223.966785	40.626240
3515.842758	372090.910241	40.631245
3515.473338	371963.390708	40.636250
3515.665919	371822.756978	40.641255
3515.598847	371684.071788	40.646260
3515.135605	371554.352617	40.651264
3515.120070	371397.469050	40.656269
3514.769850	371266.077554	40.661274
3514.800649	371120.938799	40.666279
3514.432542	370986.394729	40.671284
3514.332478	370854.835220	40.676288
3514.291913	370709.401066	40.681293
3513.958202	370576.325791	40.686298
3513.684621	370429.680954	40.691303
3513.313311	370314.495290	40.696308
3512.889503	370180.517178	40.701312
3513.101098	370050.152512	40.706317
3512.542918	369932.553080	40.711322
3512.500723	369816.067470	40.716327
3512.344703	369699.955708	40.721332
3511.812548	369572.556525	40.726336
3511.591922	369453.477748	40.731341
3511.347596	369348.878248	40.736346
3511.521126	369235.842375	40.741351
3511.054770	369141.759139	40.746356
3510.729763	369033.966070	40.751360
3510.651962	368930.458645	40.756365
3510.485934	368841.491830	40.761370
3510.190164	368740.460763	40.766375
3510.077488	368652.604544	40.771380
3509.797914	368565.486889	40.776384
3509.510003	368472.722391	40.781389
3509.463310	368383.226952	40.786394
3509.268825	368300.191389	40.791399
3509.049252	368226.801973	40.796404
3508.574960	368154.215947	40.801408
3508.916699	368071.858433	40.806413
3508.701696	368005.413485	40.811418
3508.669652	367929.653297	40.816423
3508.389035	367864.923103	40.821428
3508.072524	367794.067021	40.826432
3508.214871	367725.122750	40.831437
3507.772290	367668.788227	40.836442
3507.845897	367603.772678	40.841447
3507.841776	367545.587755	40.846452
3507.331067	367488.475073	40.851456
3507.803972	367429.883843	40.856461
3507.490409	367375.996425	40.861466
3506.979402	367316.186714	40.866471
3506.966371	367270.240461	40.871476
3506.749762	367231.450131	40.876480
3507.053185	367166.168631	40.881485
3506.971572	367120.131297	40.886490
3506.893776	367070.200656	40.891495
3506.735740	367032.800213	40.896500
3506.712946	366991.562024	40.901504
3506.759573	366940.950072	40.906509
3506.385206	366894.729802	40.911514
3506.492626	366847.186649	40.916519
3506.289575	366801.091855	40.921524
3505.963333	366767.050726	40.926528
3506.010202	366726.157473	40.931533
3505.561929	366702.414308	40.936538
3505.903779	366664.629225	40.941543
3506.637490	366638.231262	40.946548
3505.778758	366604.808477	40.951552
3505.939284	366568.196887	40.956557
3505.704445	366533.708609	40.961562
3505.661012	366490.336051	40.966567
3505.481826	366472.376563	40.971572
3505.767032	366436.584759	40.976576
3505.817047	366406.681897	40.981581
3505.657978	366380.933766	40.986586
3505.611544	366349.672213	40.991591
3505.557355	366318.182881	40.996596
3505.300524	366293.696842	41.001600
3505.511889	366251.912103	41.006605
3504.971024	366236.095993	41.011610
3505.335561	366214.361262	41.016615
3505.432208	366184.399995	41.021620
3505.280610	366161.830894	41.026624
3505.465037	366138.801578	41.031629
3505.072211	366121.817103	41.036634
3504.996744	366100.508073	41.041639
3505.164864	366071.298714	41.046644
3505.061646	366048.543808	41.051648
3505.313749	366029.498253	41.056653
3504.863358	366007.078079	41.061658
3505.340961	365974.130528	41.066663
3505.027979	365960.975235	41.071668
3504.814097	365940.120537	41.076672
3505.186559	365912.049143	41.081677
3505.009036	365902.917831	41.086682
3505.034308	365875.206613	41.091687
3505.160134	365852.720715	41.096692
3504.931043	365831.588500	41.101696
3505.028882	365805.494112	41.106701
3504.731949	365791.343958	41.111706
3505.035994	365757.889385	41.116711
3504.861203	365748.401409	41.121716
3504.734750	365726.184316	41.126720
3505.007943	365697.874051	41.131725
3504.647394	365699.432234	41.136730
3504.679012	365670.931155	41.141735
3504.637180	365646.563434	41.146740
3504.679961	365640.857491	41.151744
3504.600093	365623.696140	41.156749
3504.503173	365610.939120	41.161754
3504.789765	365585.018310	41.166759
3504.607684	365570.188412	41.171764
3504.584814	365558.691824	41.176768
3504.830620	365532.166798	41.181773
3504.479185	365523.698979	41.186778
3504.440757	365506.149386	41.191783
3504.648487	365498.865322	41.196788
3504.404732	365481.042861	41.201792
3504.559678	365459.188241	41.206797
3504.499776	365456.526236	41.211802
3504.582962	365431.833320	41.216807
3504.812402	365417.498067	41.221812
3504.399367	365410.337563	41.226816
3504.724136	365387.082134	41.231821
3504.490350	365377.476191	41.236826
3504.301050	365356.566451	41.241831
3504.469903	365343.894558	41.246836
3504.459393	365333.210139	41.251840
3504.619807	365312.524971	41.256845
3504.364239	365294.322656	41.261850
3504.502858	365280.815899	41.266855
3504.236621	365271.215063	41.271860
3504.156242	365264.281824	41.276864
3504.405720	365249.841578	41.281869
3504.348800	365243.922357	41.286874
3504.385375	365232.492618	41.291879
3504.702508	365222.697778	41.296884
3504.207157	365199.699115	41.301888
3504.506260	365182.554018	41.306893
3504.427156	365176.841841	41.311898
3504.596982	365140.634715	41.316903
3504.317880	365142.332701	41.321908
3504.240609	365125.018090	41.326912
3504.515510	365108.614646	41.331917
3504.160211	365095.287687	41.336922
3504.181692	365086.557288	41.341927
3504.499213	365067.348327	41.346932
3504.140218	365057.100583	41.351936
3504.066249	365044.238002	41.356941
3503.907327	365052.939353	41.361946
3504.319934	365026.438551	41.366951
3504.423658	365009.705925	41.371956
3504.327164	365012.062019	41.376960
3504.563592	364989.659982	41.381965
3504.177546	364966.822026	41.386970
3504.300664	364957.261347	41.391975
3504.248670	364951.443083	41.396980
3504.198224	364934.454923	41.401984
3504.211050	364928.753626	41.406989
3504.272023	364914.393959	41.411994
3504.689409	364895.779781	41.416999
3504.185946	364888.226395	41.422004
3503.847608	364880.087149	41.427008
3504.338531	364870.442865	41.432013
3504.233272	364855.193495	41.437018
3504.067849	364843.490269	41.442023
3504.028294	364836.474182	41.447028
3503.956116	364824.679880	41.452032
3503.993151	364816.964709	41.457037
3503.989171	364810.884402	41.462042
3504.111250	364799.746359	41.467047
3504.220392	364784.259524	41.472052
3504.290742	364785.317081	41.477056
3504.549149	364757.975421	41.482061
3504.256890	364747.462622	41.487066
3504.153081	364737.581561	41.492071
3504.237456	364733.777191	41.497076
3504.149257	364721.043986	41.502080
3504.349843	364700.632068	41.507085
3504.104365	364687.313072	41.512090
3503.860196	364683.357087	41.517095
3504.078840	364665.206773	41.522100
3504.056775	364663.836362	41.527104
3504.233030	364654.445324	41.532109
3503.861804	364638.779942	41.537114
3504.231255	364620.936537	41.542119
3504.155630	364606.801915	41.547124
3503.987249	364597.058250	41.552128
3504.339026	364587.715782	41.557133
3504.056859	364578.931513	41.562138
3504.350499	364562.499467	41.567143
3504.264282	364546.763555	41.572148
3504.272941	364544.853967	41.577152
3504.632421	364519.429901	41.582157
3504.074649	364518.525825	41.587162
3503.774709	364493.180544	41.592167
3503.858317	364481.081647	41.597172
3503.916195	364483.387921	41.602176
3504.090829	364469.519020	41.607181
3503.924827	364459.953054	41.612186
3504.069234	364455.324975	41.617191
3504.181628	364446.885405	41.622196
3503.943166	364443.106603	41.627200
3504.247938	364426.825411	41.632205
3504.048200	364412.277807	41.637210
3504.054964	364404.414690	41.642215
3503.818401	364397.760447	41.647220
3503.948213	364387.511610	41.652224
3504.312835	364375.724474	41.657229
3503.783349	364370.414162	41.662234
3503.927728	364367.719800	41.667239
3503.966306	364346.951679	41.672244
3504.147780	364338.475726	41.677248
3504.090475	364333.141653	41.682253
3503.969859	364320.362574	41.687258
3504.144849	364310.997110	41.692263
3504.155631	364296.416189	41.697268
3503.920843	364287.700705	41.702272
3503.987007	364281.863677	41.707277
3504.016673	364262.623553	41.712282
3504.048686	364248.649912	41.717287
3504.145192	364256.089734	41.722292
3503.881485	364230.051597	41.727296
3503.977473	364229.451268	41.732301
3503.760538	364213.227029	41.737306
3503.859019	364193.721559	41.742311
3503.924889	364195.263270	41.747316
3503.840873	364190.060623	41.752320
3504.052883	364168.094589	41.757325
3503.973972	364174.697065	41.762330
3503.830873	364156.272966	41.767335
3503.897827	364143.565961	41.772340
3504.167868	364154.693166	41.777344
3504.092071	364133.256046	41.782349
3503.844782	364125.204048	41.787354
3503.833186	364118.056211	41.792359
3503.683604	364101.261521	41.797364
3503.846470	364093.246453	41.802368
3503.890931	364084.995664	41.807373
3503.811995	364079.028884	41.812378
3503.873552	364064.414420	41.817383
3503.788234	364068.117321	41.822388
3503.556790	364062.530863	41.827392
3503.943464	364047.585115	41.832397
3503.431879	364049.192673	41.837402
3503.518751	364042.232810	41.842407
3503.572114	364056.422115	41.847412
3503.258079	364050.543385	41.852416
3503.417597	364031.842402	41.857421
3503.491829	364040.252648	41.862426
3503.526573	364037.270272	41.867431
3503.641111	364031.883555	41.872436
3503.682644	364031.851597	41.877440
3503.565298	364020.420444	41.882445
3503.392553	364017.292759	41.887450
3503.591655	364021.815795	41.892455
3503.764899	364017.615660	41.897460
3503.456341	364019.827221	41.902464
3503.750535	363999.400193	41.907469
3503.795995	363996.568784	41.912474
3503.825585	363992.569462	41.917479
3503.867150	363998.160605	41.922484
3503.346501	363979.465348	41.927488
3503.521877	363977.707489	41.932493
3503.718213	363980.119120	41.937498
3504.114050	363974.611596	41.942503
3504.102810	363958.100312	41.947508
3503.859241	363951.345335	41.952512
3504.252336	363942.428752	41.957517
3503.959421	363936.063234	41.962522
3503.970667	363916.367885	41.967527
3503.808574	363898.989888	41.972532
3503.581387	363891.367218	41.977536
3504.055223	363888.697078	41.982541
3503.647056	363875.429008	41.987546
3503.600837	363869.686026	41.992551
3503.596231	363856.990254	41.997556
3503.455173	363870.141704	42.002560
3503.677925	363863.414773	42.007565
3503.686592	363868.425920	42.012570
3503.714398	363845.700089	42.017575
3503.644802	363855.837854	42.022580
3503.756828	363844.802945	42.027584
3503.774698	363819.483383	42.032589
3503.497929	363832.147417	42.037594
3503.768765	363824.420563	42.042599
3503.766545	363810.630309	42.047604
3504.005421	363801.534527	42.052608
3503.901215	363794.146839	42.057613
3503.928887	363793.684524	42.062618
3503.732018	363775.421436	42.067623
3503.436974	363774.806585	42.072628
3503.400088	363769.418330	42.077632
3503.835595	363769.985637	42.082637
3503.144062	363766.278402	42.087642
3503.621759	363749.562529	42.092647
3503.535229	363750.059697	42.097652
3503.621286	363743.074473	42.102656
3503.640137	363748.414797	42.107661
3503.848014	363738.382472	42.112666
3504.025159	363721.968542	42.117671
3503.693588	363731.944196	42.122676
3503.529190	363724.362460	42.127680
3503.763971	363698.779546	42.132685
3503.771610	363705.979065	42.137690
3503.723162	363697.310344	42.142695
3503.774823	363684.452965	42.147700
3503.658600	363688.338891	42.152704
3503.837287	363678.412944	42.157709
3503.887267	363679.448303	42.162714
3503.626238	363667.632670	42.167719
3503.796619	363669.030657	42.172724
3503.851835	363668.436766	42.177728
3503.760047	363646.645730	42.182733
3503.349812	363637.143646	42.187738
3503.792743	363637.175454	42.192743
3504.160302	363626.608980	42.197748
3503.683542	363612.639242	42.202752
3503.801440	363596.489075	42.207757
3503.521476	363612.105195	42.212762
3503.916358	363593.544936	42.217767
3503.694932	363571.519917	42.222772
3503.938523	363569.776703	42.227776
3503.810364	363571.578105	42.232781
3503.679332	363561.344876	42.237786
3503.417774	363554.745350	42.242791
3503.810306	363542.266597	42.247796
3503.608170	363550.262627	42.252800
3503.509076	363537.021932	42.257805
3503.753555	363517.543985	42.262810
3503.537384	363526.636338	42.267815
3503.400918	363529.049715	42.272820
3503.543666	363528.823647	42.277824
3503.948579	363516.495595	42.282829
3503.559502	363505.819707	42.287834
3503.710451	363500.732502	42.292839
3503.729120	363497.523635	42.297844
3503.611777	363482.937267	42.302848
3503.830771	363475.600214	42.307853
3504.123941	363470.592300	42.312858
3503.954988	363470.542728	42.317863
3503.756206	363443.832334	42.322868
3503.478647	363441.306396	42.327872
3503.865242	363436.563596	42.332877
3503.524023	363426.490786	42.337882
3503.762486	363416.758887	42.342887
3503.629046	363405.762678	42.347892
3503.591546	363405.717769	42.352896
3503.730034	363391.777925	42.357901
3503.649766	363385.938488	42.362906
3503.741863	363379.257586	42.367911
3503.673033	363378.148971	42.372916
3503.473062	363372.150345	42.377920
3504.118669	363353.779354	42.382925
3503.691186	363350.870003	42.387930
3503.584997	363352.159055	42.392935
3503.608172	363335.820218	42.397940
3503.681858	363329.930992	42.402944
3503.853007	363330.794537	42.407949
3503.368338	363342.677353	42.412954
3503.538063	363323.007588	42.417959
3503.637777	363306.045977	42.422964
3503.476772	363307.191030	42.427968
3503.629714	363297.192739	42.432973
3503.320761	363312.609987	42.437978
3503.573845	363298.372112	42.442983
3503.638476	363287.293674	42.447988
3503.550336	363287.078660	42.452992
3503.378377	363269.523876	42.457997
3503.424344	363293.027204	42.463002
3503.461700	363273.480120	42.468007
3503.663284	363261.006033	42.473012
3503.329670	363267.776124	42.478016
3503.872074	363255.757044	42.483021
3503.643777	363252.968865	42.488026
3503.632302	363258.873814	42.493031
3503.422406	363245.854107	42.498036
3503.327488	363238.261308	42.503040
3503.637949	363232.894415	42.508045
3503.474129	363242.716433	42.513050
3503.585221	363243.182365	42.518055
3503.529789	363214.210076	42.523060
3503.450490	363218.878979	42.528064
3503.741892	363203.311912	42.533069
3503.483494	363210.833451	42.538074
3503.516674	363207.698603	42.543079
3503.714426	363195.988434	42.548084
3503.375168	363189.248473	42.553088
3503.567121	363192.627724	42.558093
3503.333554	363189.000711	42.563098
3503.599399	363194.505608	42.568103
3503.500375	363178.007922	42.573108
3503.478360	363168.368037	42.578112
3503.599955	363165.524541	42.583117
3503.414543	363168.352784	42.588122
3503.391773	363168.051103	42.593127
3503.613191	363167.125599	42.598132
3503.370343	363154.238297	42.603136
3503.569820	363146.217279	42.608141
3503.305255	363155.520909	42.613146
3503.457001	363142.291337	42.618151
3503.747632	363146.799990	42.623156
3503.426712	363143.161338	42.628160
3503.685211	363125.131340	42.633165
3503.521688	363124.419355	42.638170
3503.458464	363123.640624	42.643175
3503.637395	363128.472270	42.648180
3503.444550	363119.241046	42.653184
3503.654798	363096.791340	42.658189
3503.378458	363101.873069	42.663194
3503.313999	363099.186204	42.668199
3503.152969	363101.628930	42.673204
3502.833437	363105.343489	42.678208
3503.320781	363103.001948	42.683213
3503.562776	363106.195184	42.688218
3503.596580	363098.963680	42.693223
3503.130827	363081.557045	42.698228
3503.459040	363085.220097	42.703232
3503.654053	363075.138774	42.708237
3503.504874	363085.467399	42.713242
3503.629094	363086.211146	42.718247
3503.668613	363077.884625	42.723252
3503.526366	363061.953508	42.728256
3503.702638	363063.248805	42.733261
3503.751138	363055.811415	42.738266
3503.505238	363055.112451	42.743271
3503.702318	363030.552906	42.748276
3503.315953	363025.855923	42.753280
3503.756675	363030.493527	42.758285
3503.661727	363036.182700	42.763290
3503.684909	363018.571528	42.768295
3504.147892	363007.760828	42.773300
3503.736588	363009.963235	42.778304
3503.869424	362989.459493	42.783309
3503.492708	362979.595752	42.788314
3503.617686	362967.846142	42.793319
3503.546116	362974.040516	42.798324
3503.589861	362963.092525	42.803329
3503.628059	362947.310955	42.808333
3503.193887	362950.127647	42.813338
3503.201998	362937.073390	42.818343
3503.311852	362941.305307	42.823348
3503.418303	362955.104891	42.828353
3503.637732	362952.780250	42.833357
3503.563404	362955.590946	42.838362
3503.611856	362925.533386	42.843367
3503.818639	362920.310070	42.848372
3503.539644	362926.893464	42.853377
3503.860244	362918.140812	42.858381
3503.230642	362908.215256	42.863386
3503.193860	362899.519097	42.868391
3503.422300	362898.668811	42.873396
3503.261372	362895.284737	42.878401
3503.362058	362902.062559	42.883405
3503.203612	362909.415679	42.888410
3503.258101	362904.877993	42.893415
3503.532328	362905.877919	42.898420
3503.308361	362905.353597	42.903425
3503.645868	362877.285873	42.908429
3503.514536	362883.896820	42.913434
3503.418832	362882.537996	42.918439
3503.559899	362882.337636	42.923444
3503.351192	362890.207595	42.928449
3503.706641	362872.772842	42.933453
3503.411053	362874.244515	42.938458
3503.681462	362857.077645	42.943463
3503.782638	362854.288247	42.948468
3503.476430	362856.092379	42.953473
3503.789682	362823.804663	42.958477
3503.572522	362828.724399	42.963482
3503.484886	362833.420103	42.968487
3503.823975	362830.058758	42.973492
3503.431181	362812.411488	42.978497
3503.574149	362800.506325	42.983501
3503.430957	362806.177708	42.988506
3503.727971	362795.342307	42.993511
3503.782807	362785.868307	42.998516
3503.414693	362787.555004	43.003521
3503.750704	362773.100303	43.008525
3503.430253	362774.423242	43.013530
3503.506052	362774.156865	43.018535
3503.518671	362766.877769	43.023540
3503.639930	362756.350034	43.028545
3503.984072	362740.291028	43.033549
3503.441260	362754.549533	43.038554
3503.319831	362749.937863	43.043559
3503.460054	362729.585507	43.048564
3503.142425	362724.114289	43.053569
3503.553471	362712.573838	43.058573
3503.235888	362721.529711	43.063578
3503.563737	362721.961383	43.068583
3503.523537	362725.377368	43.073588
3503.211461	362723.467519	43.078593
3503.651350	362711.718951	43.083597
3503.490565	362701.184901	43.088602
3503.330984	362700.803065	43.093607
3503.747467	362693.002110	43.098612
3503.205872	362701.637175	43.103617
3503.310843	362693.096681	43.108621
3503.461127	362695.948219	43.113626
3503.451709	362689.283266	43.118631
3503.318271	362672.612728	43.123636
3503.346771	362672.786387	43.128641
3503.580722	362668.627423	43.133645
3503.460898	362671.038213	43.138650
3503.744173	362672.825498	43.143655
3503.894856	362659.316066	43.148660
3503.357904	362653.981290	43.153665
3503.457339	362641.853966	43.158669
3503.620348	362651.268217	43.163674
3503.466075	362642.845030	43.168679
3503.339419	362619.048896	43.173684
3503.455988	362616.257051	43.178689
3503.582338	362600.537762	43.183693
3503.186875	362617.190260	43.188698
3503.148377	362619.918978	43.193703
3503.446850	362612.543780	43.198708
3503.199632	362626.450259	43.203713
3503.182469	362606.936959	43.208717
3503.456779	362599.616468	43.213722
3503.439797	362594.326709	43.218727
3503.121257	362604.733103	43.223732
3503.288016	362610.355512	43.228737
3503.381691	362601.282449	43.233741
3503.472670	362611.420545	43.238746
3503.401658	362621.813250	43.243751
3503.635738	362607.374611	43.248756
3503.643615	362597.195545	43.253761
3503.530177	362581.107041	43.258765
3503.391802	362582.630204	43.263770
3503.640692	362576.636852	43.268775
3503.590323	362580.334347	43.273780
3503.553147	362565.302459	43.278785
3503.816936	362553.123686	43.283789
3503.378388	362561.309926	43.288794
3503.372857	362561.361742	43.293799
3503.531640	362545.662752	43.298804
3503.075500	362535.124465	43.303809
3503.362127	362535.613545	43.308813
3502.981527	362527.226116	43.313818
3503.173479	362530.605416	43.318823
3503.395528	362532.504164	43.323828
3503.195857	362534.876695	43.328833
3503.631825	362532.848584	43.333837
3503.400858	362539.780666	43.338842
3503.506474	362534.675078	43.343847
3503.514888	362515.488478	43.348852
3503.197564	362514.597238	43.353857
3503.548594	362501.335981	43.358861
3503.525853	362507.293696	43.363866
3503.441360	362512.268827	43.368871
3503.478885	362508.853353	43.373876
3503.252153	362492.350168	43.378881
3503.429277	362470.923187	43.383885
3503.075137	362479.172432	43.388890
3503.229311	362488.104662	43.393895
3503.808344	362478.573177	43.398900
3503.062973	362481.439092	43.403905
3503.538268	362487.267189	43.408909
3503.034032	362493.504580	43.413914
3503.435332	362480.973268	43.418919
3503.464941	362473.793219	43.423924
3503.151179	362461.832947	43.428929
3503.523466	362464.267733	43.433933
3503.628743	362476.693626	43.438938
3503.292083	362467.281450	43.443943
3503.359636	362482.028779	43.448948
3503.432999	362477.259065	43.453953
3503.500639	362452.796013	43.458957
3503.560776	362447.265044	43.463962
3503.341577	362442.668800	43.468967
3503.164996	362446.615260	43.473972
3502.947850	362452.145708	43.478977
3503.273402	362449.753377	43.483981
3503.229322	362450.854522	43.488986
3503.299312	362464.431011	43.493991
3503.411620	362453.599286	43.498996
3503.310565	362450.892723	43.504001
3503.194165	362429.206787	43.509005
3503.073032	362433.602489	43.514010
3503.248421	362429.300092	43.519015
3503.673652	362433.456755	43.524020
3503.634394	362437.966737	43.529025
3503.340353	362425.748891	43.534029
3503.217363	362431.697018	43.539034
3503.401166	362428.512861	43.544039
3503.458710	362414.305629	43.549044
3503.465921	362415.220553	43.554049
3503.350072	362401.524178	43.559053
3503.360375	362408.469028	43.564058
3503.634855	362405.932100	43.569063
3503.659115	362397.404312	43.574068
3503.023206	362393.255609	43.579073
3503.630363	362380.818952	43.584077
3503.185820	362389.896738	43.589082
3503.348386	362376.029118	43.594087
3503.726971	362382.788529	43.599092
3503.649053	362384.734703	43.604097
3503.419332	362358.893701	43.609101
3503.270700	362361.461731	43.614106
3503.471497	362355.221505	43.619111
3503.543460	362356.355197	43.624116
3503.179669	362361.578055	43.629121
3503.255469	362358.156519	43.634125
3503.415879	362357.011641	43.639130
3503.315929	362345.068429	43.644135
3503.322624	362332.268675	43.649140
3503.141192	362326.546876	43.654145
3503.413926	362320.982284	43.659149
3503.391769	362334.878716	43.664154
3503.644892	362330.665802	43.669159
3503.537970	362326.764252	43.674164
3503.427144	362330.038762	43.679169
3503.747620	362297.520538	43.684173
3503.477131	362301.303742	43.689178
3503.406000	362303.681408	43.694183
3503.455692	362308.304566	43.699188
3503.633650	362297.589651	43.704193
3503.602166	362271.411924	43.709197
3503.452478	362278.102192	43.714202
3503.312025	362273.951491	43.719207
3503.749117	362275.892589	43.724212
3503.257540	362269.252908	43.729217
3503.580824	362245.716240	43.734221
3503.432510	362245.281729	43.739226
3503.334156	362233.440016	43.744231
3503.588779	362237.038434	43.749236
3503.591711	362235.613108	43.754241
3503.796918	362240.338913	43.759245
3503.688971	362221.603150	43.764250
3503.624713	362218.610863	43.769255
3503.514079	362212.139957	43.774260
3503.245312	362206.381060	43.779265
3503.448639	362202.608569	43.784269
3503.584320	362190.399064	43.789274
3503.455094	362176.170394	43.794279
3503.345824	362180.869584	43.799284
3503.328543	362181.075927	43.804289
3503.785558	362174.260830	43.809293
3502.978622	362175.864250	43.814298
3503.198907	362150.180999	43.819303
3503.513032	362138.630284	43.824308
3503.255377	362150.070395	43.829313
3503.642091	362152.706476	43.834317
3503.632384	362149.629226	43.839322
3503.667599	362148.453244	43.844327
3503.534284	362133.487306	43.849332
3503.229933	362131.219981	43.854337
3503.573970	362118.468621	43.859341
3503.306812	362119.096139	43.864346
3503.426456	362122.359675	43.869351
3503.503858	362126.596796	43.874356
3503.360049	362110.512932	43.879361
3503.727855	362097.045349	43.884365
3503.450956	362098.564982	43.889370
3503.301627	362087.062074	43.894375
3503.308403	362091.157693	43.899380
3503.455984	362100.625383	43.904385
3503.453247	362084.468319	43.909389
3503.147128	362069.122558	43.914394
3503.268021	362058.518390	43.919399
3503.355888	362057.613977	43.924404
3503.174111	362065.021807	43.929409
3503.392175	362059.720277	43.934413
3503.116171	362067.448342	43.939418
3503.311355	362064.669481	43.944423
3503.477795	362070.775460	43.949428
3503.165969	362071.639045	43.954433
3503.498487	362064.996284	43.959437
3503.427169	362062.615782	43.964442
3503.503222	362058.812509	43.969447
3503.517629	362055.756886	43.974452
3503.444224	362054.648963	43.979457
3503.564279	362056.029510	43.984461
3503.459327	362064.901004	43.989466
3503.684916	362040.005649	43.994471
3503.725771	362025.241147	43.999476
3503.292495	362026.073043	44.004481
3503.525207	362017.486787	44.009485
3503.366215	362016.214278	44.014490
3503.123111	361993.632150	44.019495
3503.684392	361993.976038	44.024500
3503.392810	361988.118941	44.029505
3503.366548	361987.436129	44.034509
3503.412467	361988.319497	44.039514
3503.322704	361984.262536	44.044519
3503.650187	361984.617939	44.049524
3503.280677	361975.185411	44.054529
3503.507912	361964.182735	44.059533
3503.168991	361960.088825	44.064538
3503.499775	361956.703286	44.069543
3503.544441	361963.897221	44.074548
3503.529292	361966.545950	44.079553
3503.690709	361947.487601	44.084557
3503.725918	361944.428682	44.089562
3503.556284	361941.631150	44.094567
3503.645870	361940.014003	44.099572
3503.111940	361930.734684	44.104577
3503.563294	361902.241259	44.109581
3503.008570	361905.560526	44.114586
3502.766134	361896.464126	44.119591
3503.236598	361902.674735	44.124596
3503.022884	361896.703537	44.129601
3503.309080	361902.256260	44.134605
3502.939404	361909.464813	44.139610
3503.169097	361913.016307	44.144615
3503.298307	361911.240223	44.149620
3503.055604	361913.263357	44.154625
3503.378097	361904.790114	44.159629
3503.271361	361916.995220	44.164634
3503.237292	361911.122850	44.169639
3503.100188	361920.177570	44.174644
3503.214949	361924.536028	44.179649
3503.481484	361917.649227	44.184653
3503.118292	361917.554023	44.189658
3503.231909	361912.930558	44.194663
3503.211066	361893.951890	44.199668
3502.881144	361898.914994	44.204673
3503.378728	361892.398785	44.209677
3503.310232	361885.743057	44.214682
3503.297975	361897.246216	44.219687
3503.194795	361896.499227	44.224692
3503.226222	361899.802169	44.229697
3503.330427	361896.834120	44.234701
3503.022971	361909.986982	44.239706
3503.261770	361904.783936	44.244711
3503.521796	361906.498591	44.249716
3503.107590	361899.235944	44.254721
3503.472852	361890.883163	44.259725
3503.413638	361882.139472	44.264730
3503.463849	361877.780478	44.269735
3503.261302	361882.621668	44.274740
3503.352472	361880.495366	44.279745
3503.359624	361874.565585	44.284749
3503.211696	361887.413338	44.289754
3503.258754	361887.202390	44.294759
3503.353508	361861.996838	44.299764
3503.120196	361860.507067	44.304769
3503.642619	361857.956359	44.309773
3503.416977	361851.147353	44.314778
3503.481379	361853.020160	44.319783
3503.370368	361862.248882	44.324788
3503.289153	361850.913264	44.329793
3503.491796	361833.680398	44.334797
3503.174123	361838.361676	44.339802
3503.426023	361813.309371	44.344807
3503.784213	361821.344343	44.349812
3503.370735	361814.870366	44.354817
3503.498440	361819.786580	44.359821
3502.974732	361826.536039	44.364826
3502.977246	361822.591702	44.369831
3503.461653	361834.779715	44.374836
3503.080684	361810.565363	44.379841
3503.402926	361796.799557	44.384845
3503.305477	361800.606336	44.389850
3503.504381	361807.317899	44.394855
3503.301653	361795.416240	44.399860
3503.509469	361800.599688	44.404865
3503.575504	361791.174607	44.409869
3503.211319	361781.868425	44.414874
3503.348406	361759.963992	44.419879
3503.588416	361769.315357	44.424884
3503.541942	361764.589961	44.429889
3503.791058	361773.380092	44.434893
3503.482080	361771.189817	44.439898
3503.321402	361754.192473	44.444903
3503.393054	361748.863163	44.449908
3503.459057	361750.201373	44.454913
3503.538692	361742.860634	44.459917
3503.282861	361744.605953	44.464922
3503.388318	361741.001568	44.469927
3503.436049	361742.291777	44.474932
3503.328846	361724.319053	44.479937
3503.683398	361712.023934	44.484941
3503.417859	361706.417136	44.489946
3503.720862	361706.674630	44.494951
3503.695607	361704.464945	44.499956
3503.470911	361689.920434	44.504961
3503.457778	361683.841164	44.509965
3503.365475	361684.262930	44.514970
3503.536896	361678.408937	44.519975
3503.475806	361688.265930	44.524980
3503.140557	361682.390253	44.529985
3503.310622	361655.900426	44.534989
3502.934116	361645.094898	44.539994
3502.879175	361656.350412	44.544999
3503.381905	361648.968219	44.550004
3503.185831	361648.414027	44.555009
3503.219909	361650.851431	44.560013
3503.248223	361656.979298	44.565018
3503.234661	361655.963686	44.570023
3503.642834	361656.967910	44.575028
3503.407221	361658.964489	44.580033
3503.681737	361661.414773	44.585037
3503.760154	361640.791819	44.590042
3503.334881	361636.431634	44.595047
3503.707916	361641.512646	44.600052
3503.224584	361639.400817	44.605057
3503.447533	361643.716753	44.610061
3503.515902	361630.754388	44.615066
3503.165160	361619.359542	44.620071
3503.510264	361606.251642	44.625076
3503.072123	361608.153012	44.630081
3503.326509	361595.721026	44.635085
3503.227241	361608.586608	44.640090
3503.404717	361608.685830	44.645095
3503.703192	361603.829551	44.650100
3503.609816	361594.531412	44.655105
3503.424453	361578.377599	44.660109
3503.305827	361572.671225	44.665114
3503.190040	361570.857524	44.670119
3503.811255	361569.894234	44.675124
3503.186027	361574.776828	44.680129
3503.434982	361574.355846	44.685133
3503.409086	361568.075017	44.690138
3503.431871	361561.150361	44.695143
3503.595297	361542.829443	44.700148
3502.922633	361546.472722	44.705153
3503.485546	361546.231115	44.710157
3503.373816	361547.724654	44.715162
3503.298739	361547.889246	44.720167
3503.394132	361554.489982	44.725172
3503.093058	361541.585995	44.730177
3503.422394	361521.483119	44.735181
3503.364965	361517.599124	44.740186
3503.375798	361525.002035	44.745191
3503.305692	361517.634042	44.750196
3503.360718	361517.956184	44.755201
3503.576038	361520.593950	44.760205
3503.471718	361515.903118	44.765210
3503.021889	361491.394145	44.770215
3503.233504	361490.190260	44.775220
3503.123189	361488.910042	44.780225
3503.215150	361482.432453	44.785229
3503.211322	361492.509443	44.790234
3503.007163	361491.600293	44.795239
3503.231294	361484.669241	44.800244
3503.169898	361495.620470	44.805249
3503.362767	361487.523878	44.810253
3503.174894	361498.495100	44.815258
3503.046446	361498.846246	44.820263
3503.548782	361498.995894	44.825268
3503.309638	361506.972677	44.830273
3503.278098	361484.662204	44.835277
3503.096685	361481.433937	44.840282
3503.500494	361463.838347	44.845287
3503.694173	361467.751802	44.850292
3503.555658	361473.269934	44.855297
3503.852769	361465.436758	44.860301
3503.196427	361461.367537	44.865306
3503.179452	361446.611997	44.870311
3503.305304	361427.864405	44.875316
3503.092943	361437.490911	44.880321
3503.454679	361431.326903	44.885325
3503.377619	361440.168659	44.890330
3503.493771	361437.376811	44.895335
3503.298203	361438.578263	44.900340
3503.505484	361441.420867	44.905345
3503.549834	361423.882086	44.910349
3503.016587	361414.831565	44.915354
3503.231560	361414.212391	44.920359
3503.378513	361406.352051	44.925364
3503.291495	361424.610156	44.930369
3503.277833	361412.398613	44.935373
3503.176065	361409.513985	44.940378
3503.230563	361420.090676	44.945383
3503.149781	361416.922833	44.950388
3503.124470	361426.774224	44.955393
3503.745361	361404.869482	44.960397
3503.668816	361402.846008	44.965402
3503.549039	361383.755548	44.970407
3503.433323	361381.203913	44.975412
3503.471468	361374.327692	44.980417
3503.646359	361380.864995	44.985421
3503.240131	361350.801971	44.990426
3503.461132	361352.395588	44.995431
3503.531740	361343.605829	45.000436
3503.285896	361350.387765	45.005441
3503.155689	361344.581413	45.010445
3503.186763	361356.612207	45.015450
3503.183424	361354.602603	45.020455
3503.336564	361347.453746	45.025460
3503.197314	361345.262064	45.030465
3503.436709	361324.028281	45.035469
3503.211309	361326.939292	45.040474
3503.151511	361318.450042	45.045479
3503.127468	361316.927173	45.050484
3503.216097	361335.666451	45.055489
3503.275329	361311.967498	45.060493
3503.301501	361320.080488	45.065498
3503.370816	361329.637041	45.070503
3503.591893	361324.182280	45.075508
3503.190902	361317.070127	45.080513
3503.335402	361296.538358	45.085517
3503.121039	361301.635929	45.090522
3503.293638	361299.038712	45.095527
3503.210212	361301.138473	45.100532
3503.306365	361305.957947	45.105537
3503.229821	361306.453562	45.110541
3503.237034	361304.213279	45.115546
3503.245513	361301.947352	45.120551
3503.430185	361298.075956	45.125556
3503.237252	361292.762976	45.130561
3503.191873	361283.228180	45.135565
3503.041623	361275.643811	45.140570
3503.224766	361274.088186	45.145575
3503.466223	361264.228143	45.150580
3503.077862	361268.233625	45.155585
3503.421680	361258.331953	45.160589
3503.345802	361261.601012	45.165594
3503.244835	361271.998749	45.170599
3503.390768	361273.248001	45.175604
3503.322402	361272.699062	45.180609
3503.402495	361272.228435	45.185613
3503.513005	361264.119379	45.190618
3503.132292	361244.561205	45.195623
3503.423043	361236.907114	45.200628
3503.089408	361244.975214	45.205633
3503.421669	361239.350195	45.210637
3503.294709	361241.227832	45.215642
3503.117643	361240.238058	45.220647
3503.440115	361248.813128	45.225652
3503.275515	361250.365925	45.230657
3503.336399	361228.575074	45.235661
3503.321514	361215.065958	45.240666
3502.957802	361205.047115	45.245671
3503.378255	361203.199519	45.250676
3502.994629	361219.570738	45.255681
3503.187080	361208.955067	45.260685
3503.028579	361220.176165	45.265690
3503.374043	361215.973999	45.270695
3503.291754	361222.653761	45.275700
3503.264020	361220.419000	45.280705
3503.249588	361220.090543	45.285709
3502.885380	361225.949727	45.290714
3503.186989	361230.838511	45.295719
3503.373035	361219.842174	45.300724
3502.913204	361223.095596	45.305729
3503.363720	361225.492634	45.310733
3503.055686	361210.528578	45.315738
3503.012500	361215.319198	45.320743
3503.229544	361205.259438	45.325748
3503.024355	361212.213085	45.330753
3503.449480	361205.810018	45.335757
3503.077748	361209.202186	45.340762
3503.478219	361206.747059	45.345767
3503.444030	361204.207972	45.350772
3503.082509	361222.382321	45.355777
3503.148400	361211.913885	45.360781
3503.550726	361211.061527	45.365786
3503.141976	361218.225471	45.370791
3503.545443	361199.255784	45.375796
3503.205512	361189.131397	45.380801
3503.546620	361178.924791	45.385805
3503.084361	361178.921582	45.390810
3502.906392	361178.669868	45.395815
3503.196527	361173.840309	45.400820
3503.014114	361176.540970	45.405825
3503.094583	361174.238210	45.410829
3503.338327	361182.342274	45.415834
3503.217281	361177.781280	45.420839
3503.314856	361184.229051	45.425844
3503.050948	361192.540591	45.430849
3503.202295	361181.804185	45.435853
3503.335951	361195.981666	45.440858
3503.078817	361187.727152	45.445863
3503.282888	361162.656619	45.450868
3503.130068	361158.965792	45.455873
3503.217484	361155.593223	45.460877
3503.200392	361154.883504	45.465882
3503.174392	361157.584885	45.470887
3503.166858	361161.301165	45.475892
3503.162306	361161.759954	45.480897
3503.263171	361160.700797	45.485901
3503.288235	361164.819051	45.490906
3502.984636	361165.197887	45.495911
3503.398735	361171.086713	45.500916
3503.006117	361174.609413	45.505921
3503.448363	361176.931425	45.510925
3503.154860	361183.441019	45.515930
3503.158931	361183.440427	45.520935
3503.142115	361164.664393	45.525940
3503.296117	361144.232839	45.530945
3503.188212	361146.234695	45.535949
3503.211661	361139.564327	45.540954
3502.981756	361141.738142	45.545959
3503.252214	361135.206844	45.550964
3503.350342	361140.814832	45.555969
3503.266189	361142.125906	45.560973
3503.492861	361147.102882	45.565978
3503.326392	361143.923121	45.570983
3503.343296	361149.060484	45.575988
3503.059561	361150.224990	45.580993
3503.391500	361134.370931	45.585997
3503.048332	361122.847541	45.591002
3503.383334	361120.631768	45.596007
3503.089057	361109.405991	45.601012
3502.916048	361111.723486	45.606017
3503.038130	361116.335317	45.611021
3503.191851	361120.280563	45.616026
3503.188949	361125.802742	45.621031
3503.416040	361121.950073	45.626036
3503.266938	361122.711614	45.631041
3503.504385	361120.816609	45.636045
3503.471864	361117.641117	45.641050
3503.347350	361117.075606	45.646055
3503.492726	361092.065205	45.651060
3503.351807	361087.990809	45.656065
3503.336378	361084.761722	45.661069
3503.166924	361079.801243	45.666074
3503.382328	361090.505243	45.671079
3503.393174	361084.651116	45.676084
3503.033901	361100.051597	45.681089
3503.302187	361086.726688	45.686093
3503.144400	361098.125820	45.691098
3503.198423	361093.664370	45.696103
3503.509678	361069.441991	45.701108
3503.345732	361061.808861	45.706113
3503.338191	361052.929621	45.711117
3503.368984	361064.756968	45.716122
3503.336669	361054.965606	45.721127
3503.448246	361054.693564	45.726132
3503.315731	361056.164958	45.731137
3503.891037	361045.972193	45.736141
3503.615411	361038.000477	45.741146
3503.306808	361042.807627	45.746151
3503.700235	361030.226285	45.751156
3503.362271	361030.356100	45.756161
3503.428079	361020.014863	45.761165
3503.592158	361014.569077	45.766170
3503.642542	361003.645027	45.771175
3503.450033	360997.059669	45.776180
3503.221587	361000.174746	45.781185
3503.304356	361000.059931	45.786189
3503.383781	360991.777624	45.791194
3503.040038	360981.755577	45.796199
3502.998266	360959.192020	45.801204
3502.945362	360961.057961	45.806209
3503.354985	360950.407901	45.811213
3503.216950	360970.328207	45.816218
3503.075849	360963.378480	45.821223
3503.477034	360961.101347	45.826228
3503.295013	360967.618792	45.831233
3503.475862	360965.758174	45.836237
3503.495112	360965.449835	45.841242
3503.173712	360967.587231	45.846247
3503.385496	360960.454491	45.851252
3502.836704	360938.403650	45.856257
3503.109211	360936.961116	45.861261
3503.099343	360938.540353	45.866266
3502.871678	360939.212535	45.871271
3503.321878	360927.589123	45.876276
3502.944332	360940.422540	45.881281
3503.071463	360935.491498	45.886285
3503.021804	360937.484155	45.891290
3503.504561	360941.453738	45.896295
3503.333203	360943.160286	45.901300
3502.933456	360942.358382	45.906305
3503.142128	360938.050589	45.911309
3503.032343	360945.421767	45.916314
3502.930685	360943.631254	45.921319
3503.304857	360941.943638	45.926324
3503.197164	360947.406067	45.931329
3503.398985	360942.132426	45.936333
3503.440407	360949.199799	45.941338
3503.870464	360955.493258	45.946343
3503.728922	360933.454372	45.951348
3503.588796	360919.354276	45.956353
3503.441752	360918.257967	45.961357
3502.999011	360927.132182	45.966362
3503.018756	360924.813564	45.971367
3503.512343	360913.005171	45.976372
3503.403255	360904.192847	45.981377
3503.567950	360895.922489	45.986381
3503.548733	360891.498044	45.991386
3503.280626	360889.784732	45.996391
3503.123041	360892.685049	46.001396
3502.960399	360895.051807	46.006401
3503.537707	360883.713638	46.011405
3503.225444	360888.394154	46.016410
3503.368787	360880.330734	46.021415
3503.393494	360852.845614	46.026420
3503.385321	360849.335462	46.031425
3503.542413	360846.282650	46.036429
3503.279900	360852.482042	46.041434
3503.409611	360853.097729	46.046439
3503.595829	360857.597663	46.051444
3503.512084	360851.987471	46.056449
3503.485692	360820.617230	46.061453
3503.502628	360823.184614	46.066458
3503.349834	360828.908643	46.071463
3503.353708	360820.383794	46.076468
3503.170514	360825.527379	46.081473
3503.740849	360827.905497	46.086477
3503.505913	360806.186663	46.091482
3503.621182	360795.277754	46.096487
3503.340919	360789.291490	46.101492
3503.122403	360784.923987	46.106497
3503.808366	360784.179457	46.111501
3503.571722	360783.326321	46.116506
3503.564919	360770.808181	46.121511
3503.968627	360753.365019	46.126516
3503.521361	360759.008379	46.131521
3503.641574	360750.694137	46.136525
3503.498693	360730.054881	46.141530
3503.311521	360716.013053	46.146535
3503.695637	360707.453519	46.151540
3503.317579	360708.454826	46.156545
3503.428923	360711.058183	46.161549
3503.750129	360719.658994	46.166554
3503.423374	360696.504222	46.171559
3503.224567	360683.074921	46.176564
3503.223298	360685.492516	46.181569
3503.189396	360685.039904	46.186573
3503.249521	360673.223639	46.191578
3503.341513	360678.043834	46.196583
3503.477702	360675.146991	46.201588
3503.309852	360680.364503	46.206593
3503.544573	360650.454170	46.211597
3503.332472	360642.039768	46.216602
3503.072688	360645.363387	46.221607
3503.353236	360646.235135	46.226612
3502.946597	360651.464953	46.231617
3503.127106	360645.075036	46.236621
3503.323691	360655.298641	46.241626
3503.153817	360656.648724	46.246631
3502.954708	360643.677483	46.251636
3503.129210	360656.474598	46.256641
3503.078091	360657.526005	46.261645
3503.176111	360656.365504	46.266650
3502.896183	360655.544653	46.271655
3503.227340	360656.001268	46.276660
3503.383342	360657.121716	46.281665
3503.165534	360656.723623	46.286669
3503.066604	360641.344646	46.291674
3503.147819	360634.130715	46.296679
3503.383269	360615.721718	46.301684
3503.241505	360633.098178	46.306689
3503.253486	360626.785792	46.311693
3503.260436	360626.835636	46.316698
3503.047783	360629.973686	46.321703
3503.122614	360629.911016	46.326708
3502.982921	360629.653248	46.331713
3503.255570	360626.734829	46.336717
3503.266118	360628.896101	46.341722
3503.157345	360634.104280	46.346727
3503.629246	360636.243511	46.351732
3503.226376	360642.694130	46.356737
3503.714345	360607.883600	46.361741
3503.511347	360610.256751	46.366746
3503.090947	360604.190835	46.371751
3503.329246	360593.440551	46.376756
3503.568213	360604.369948	46.381761
3503.183990	360603.998161	46.386765
3503.158667	360599.371088	46.391770
3503.365352	360590.508787	46.396775
3503.554310	360571.318304	46.401780
3503.115167	360571.591343	46.406785
3503.131111	360559.273119	46.411789
3503.392777	360567.323562	46.416794
3503.575639	360565.564394	46.421799
3503.213186	360567.504731	46.426804
3503.293174	360567.822933	46.431809
3503.562372	360571.393728	46.436813
3503.409808	360550.297901	46.441818
3503.277561	360540.649460	46.446823
3503.656490	360531.123775	46.451828
3503.394068	360535.923674	46.456833
3503.186997	360526.821420	46.461837
3503.286740	360526.831150	46.466842
3503.359569	360538.626537	46.471847
3503.396146	360537.908324	46.476852
3503.201093	360511.857268	46.481857
3503.165431	360505.247047	46.486861
3503.015557	360498.985677	46.491866
3503.064063	360504.143560	46.496871
3503.493484	360496.900008	46.501876
3503.304175	360500.594183	46.506881
3503.093073	360503.273971	46.511885
3503.379710	360504.373772	46.516890
3503.143067	360503.520629	46.521895
3503.405092	360507.245239	46.526900
3503.176020	360503.744536	46.531905
3503.688336	360490.660788	46.536909
3503.431186	360476.757182	46.541914
3503.154604	360475.910353	46.546919
3503.695881	360467.478606	46.551924
3503.066278	360472.692799	46.556929
3503.118501	360474.109561	46.561933
3503.016595	360472.064611	46.566938
3503.457591	360474.386856	46.571943
3503.411796	360473.045518	46.576948
3503.114717	360468.588622	46.581953
3503.084433	360453.198733	46.586957
3503.252348	360438.159194	46.591962
3503.013596	360453.108251	46.596967
3503.205984	360436.283634	46.601972
3503.183931	360455.066202	46.606977
3503.080606	360448.237658	46.611981
3503.141532	360441.510376	46.616986
3503.346114	360444.658817	46.621991
3503.308239	360448.965203	46.626996
3502.882586	360450.228498	46.632001
3503.288326	360440.418652	46.637005
3503.311376	360450.109925	46.642010
3503.298122	360461.231901	46.647015
3503.365755	360454.427224	46.652020
3503.356050	360459.543422	46.657025
3503.090254	360433.528952	46.662029
3503.538139	360430.455590	46.667034
3503.491070	360427.893052	46.672039
3503.154715	360423.696819	46.677044
3503.177477	360420.588879	46.682049
3503.317076	360415.045111	46.687053
3503.295379	360416.269994	46.692058
3502.968692	360423.268408	46.697063
3503.104953	360413.959182	46.702068
3503.249331	360424.496439	46.707073
3503.323855	360417.334425	46.712077
3503.532072	360427.581685	46.717082
3503.470899	360399.117493	46.722087
3503.573328	360392.536319	46.727092
3503.243187	360395.311268	46.732097
3503.373471	360397.580852	46.737101
3503.302878	360399.144261	46.742106
3503.112282	360406.680973	46.747111
3503.322379	360389.497298	46.752116
3503.201675	360394.503821	46.757121
3503.301243	360365.785186	46.762125
3503.433194	360359.224786	46.767130
3503.000307	360348.758673	46.772135
3503.179025	360355.168282	46.777140
3503.130530	360359.807151	46.782145
3503.107595	360348.411070	46.787149
3502.876648	360357.837164	46.792154
3502.939630	360360.600861	46.797159
3503.095786	360344.468979	46.802164
3502.982081	360361.561197	46.807169
3502.966605	360365.965833	46.812173
3502.865735	360374.328080	46.817178
3503.066188	360374.907144	46.822183
3503.329537	360363.389472	46.827188
3502.904444	360365.695962	46.832193
3502.848697	360356.111728	46.837197
3502.992225	360364.155435	46.842202
3502.841005	360371.278794	46.847207
3503.137236	360373.598483	46.852212
3503.110554	360373.551860	46.857217
3503.409981	360364.725749	46.862221
3503.416977	360379.203400	46.867226
3503.170083	360383.797293	46.872231
3503.472430	360379.372858	46.877236
3503.164916	360383.162066	46.882241
3503.233918	360381.217323	46.887245
3503.377460	360384.197296	46.892250
3503.049362	360363.078244	46.897255
3503.293039	360343.548223	46.902260
3503.309757	360346.446464	46.907265
3503.565212	360346.889604	46.912269
3503.270628	360342.432302	46.917274
3503.313456	360345.479090	46.922279
3503.667594	360335.066679	46.927284
3503.413064	360331.061070	46.932289
3503.252713	360309.788247	46.937293
3503.504778	360312.216704	46.942298
3503.283412	360314.058410	46.947303
3503.275159	360307.520167	46.952308
3503.166839	360320.234851	46.957313
3503.180036	360316.492268	46.962317
3503.176674	360318.299511	46.967322
3503.044876	360322.468081	46.972327
3503.166751	360319.827937	46.977332
3503.054337	360321.728757	46.982337
3503.251487	360321.010603	46.987341
3503.117806	360317.316685	46.992346
3503.099875	360320.398526	46.997351
3503.150700	360308.176507	47.002356
3503.077747	360303.862285	47.007361
3503.541793	360297.732851	47.012365
3503.344868	360300.359517	47.017370
3503.343001	360299.901837	47.022375
3503.703809	360281.905476	47.027380
3503.263852	360292.865933	47.032385
3503.511246	360299.849949	47.037389
3503.640579	360285.910637	47.042394
3503.435817	360272.049581	47.047399
3503.445242	360256.373446	47.052404
3503.086785	360263.605919	47.057409
3503.138460	360253.877453	47.062413
3503.191760	360266.897399	47.067418
3503.154724	360251.025039	47.072423
3503.546283	360246.942733	47.077428
3503.406354	360260.909281	47.082433
3503.315125	360240.796013	47.087437
3503.452080	360224.132761	47.092442
3503.206948	360223.535415	47.097447
3503.352627	360222.647275	47.102452
3503.237072	360221.113391	47.107457
3503.438079	360218.333503	47.112461
3503.157057	360222.322103	47.117466
3503.313511	360228.429897	47.122471
3503.303220	360231.281523	47.127476
3503.125335	360206.321762	47.132481
3502.826396	360195.859886	47.137485
3503.149274	360205.707378	47.142490
3503.059519	360200.377965	47.147495
3503.318604	360200.362506	47.152500
3502.970578	360191.791390	47.157505
3503.009400	360193.973658	47.162509
3502.915564	360194.828261	47.167514
3502.994361	360193.798017	47.172519
3503.549107	360187.018081	47.177524
3502.991768	360196.826601	47.182529
3503.038248	360193.078747	47.187533
3503.119291	360194.948989	47.192538
3502.866416	360195.370706	47.197543
3503.131799	360185.812010	47.202548
3503.124079	360203.676355	47.207553
3503.323207	360192.397809	47.212557
3503.274940	360197.952713	47.217562
3503.217237	360206.460840	47.222567
3503.351063	360203.360774	47.227572
3503.258539	360204.749534	47.232577
3503.163706	360202.703454	47.237581
3503.113103	360209.276565	47.242586
3503.376854	360202.822538	47.247591
3503.327880	360190.539927	47.252596
3502.991024	360183.951830	47.257601
3503.310681	360173.468497	47.262605
3503.195939	360175.115231	47.267610
3503.014251	360173.566353	47.272615
3503.093845	360170.067722	47.277620
3503.167123	360173.618628	47.282625
3503.114743	360179.733996	47.287629
3503.424665	360188.413024	47.292634
3502.943553	360180.422757	47.297639
3503.161783	360183.060138	47.302644
3502.759064	360184.243476	47.307649
3503.356453	360167.685539	47.312653
3503.284369	360176.552189	47.317658
3503.137427	360183.496776	47.322663
3503.068724	360180.937645	47.327668
3503.341947	360190.385854	47.332673
3503.100440	360193.121358	47.337677
3503.238411	360192.565233	47.342682
3503.057077	360184.807482	47.347687
3503.330447	360170.081986	47.352692
3503.003157	360158.454068	47.357697
3503.174154	360153.872255	47.362701
3503.099241	360146.224905	47.367706
3503.114010	360152.075201	47.372711
3503.111496	360143.144105	47.377716
3503.025701	360154.506634	47.382721
3503.231613	360155.008500	47.387725
3503.306279	360160.238623	47.392730
3503.146222	360153.648019	47.397735
3503.473891	360147.412894	47.402740
3503.008038	360156.010998	47.407745
3503.367847	360157.175577	47.412749
3503.114665	360150.497911	47.417754
3503.082983	360159.917988	47.422759
3503.432371	360156.071354	47.427764
3503.273534	360143.220841	47.432769
3503.254509	360120.856861	47.437773
3503.154649	360124.536925	47.442778
3503.314139	360112.806598	47.447783
3503.520060	360112.036162	47.452788
3503.281884	360128.003069	47.457793
3503.284852	360117.697017	47.462797
3503.279249	360124.161242	47.467802
3503.150471	360118.710759	47.472807
3503.506698	360125.932056	47.477812
3503.076720	360107.907964	47.482817
3503.010442	360097.892761	47.487821
3503.158547	360100.261325	47.492826
3503.191908	360097.482487	47.497831
3503.588561	360087.572221	47.502836
3503.193002	360104.378289	47.507841
3503.224345	360093.940516	47.512845
3503.202813	360089.872608	47.517850
3503.122140	360107.341385	47.522855
3503.290868	360098.001519	47.527860
3503.401887	360099.205430	47.532865
3503.492843	360091.099267	47.537869
3503.457328	360076.702479	47.542874
3503.395440	360072.640948	47.547879
3503.766401	360062.582063	47.552884
3503.318281	360069.523386	47.557889
3503.429303	360070.091146	47.562893
3503.433749	360063.220064	47.567898
3503.252300	360044.291495	47.572903
3503.477374	360027.105323	47.577908
3503.228707	360022.411718	47.582913
3503.312657	360014.204865	47.587917
3503.258466	360022.432563	47.592922
3503.088803	360024.724135	47.597927
3503.172162	360018.044140	47.602932
3503.090886	360033.273785	47.607937
3503.313034	360021.151840	47.612941
3503.396442	360028.263604	47.617946
3503.233082	360022.894914	47.622951
3503.217075	360016.128843	47.627956
3503.167277	360010.767647	47.632961
3503.478442	360001.176231	47.637965
3503.255575	360000.880715	47.642970
3503.120298	359999.604402	47.647975
3503.375977	359995.925246	47.652980
3503.376119	359996.205182	47.657985
3503.653106	359994.278437	47.662989
3503.331079	359992.955308	47.667994
3503.449745	359984.463055	47.672999
3503.187627	359966.743173	47.678004
3503.256065	359964.391365	47.683009
3503.016502	359962.291816	47.688013
3503.102750	359953.753791	47.693018
3502.874371	359962.441619	47.698023
3503.176949	359960.816179	47.703028
3503.107103	359973.855672	47.708033
3503.195629	359965.648088	47.713037
3503.223284	359973.404826	47.718042
3503.198261	359979.668571	47.723047
3503.394257	359974.395745	47.728052
3502.925812	359974.317173	47.733057
3503.314078	359975.222798	47.738061
3503.277480	359969.401480	47.743066
3503.264557	359978.131584	47.748071
3503.459056	359964.410891	47.753076
3503.090625	359950.830077	47.758081
3503.400810	359949.025313	47.763085
3503.147960	359942.474795	47.768090
3503.209898	359941.778010	47.773095
3503.198220	359945.469593	47.778100
3503.038165	359949.591770	47.783105
3503.120960	359942.504716	47.788109
3503.153296	359941.278243	47.793114
3503.000193	359948.732760	47.798119
3503.473234	359940.947862	47.803124
3503.037828	359948.167100	47.808129
3502.855619	359947.407126	47.813133
3503.019919	359954.862359	47.818138
3502.832856	359945.069787	47.823143
3503.262935	359936.197497	47.828148
3502.990103	359953.620368	47.833153
3503.450940	359944.157957	47.838157
3503.573733	359952.103227	47.843162
3502.911910	359944.370503	47.848167
3503.382012	359932.845490	47.853172
3503.204988	359930.532484	47.858177
3503.162724	359923.210736	47.863181
3502.961189	359915.176228	47.868186
3502.852869	359917.178201	47.873191
3503.198788	359911.652652	47.878196
3502.917984	359926.659412	47.883201
3503.091129	359918.820134	47.888205
3503.193787	359923.867735	47.893210
3502.744701	359928.493634	47.898215
3502.989549	359924.205478	47.903220
3503.338018	359923.641520	47.908225
3503.195129	359926.336003	47.913229
3503.157723	359919.217055	47.918234
3503.113959	359920.470885	47.923239
3503.315857	359918.861360	47.928244
3503.059527	359934.602186	47.933249
3503.134547	359925.429778	47.938253
3503.076074	359926.278795	47.943258
3502.994327	359931.508223	47.948263
3503.183592	359930.129711	47.953268
3502.963381	359928.332454	47.958273
3502.989688	359930.567605	47.963277
3502.985874	359935.581143	47.968282
3502.962297	359933.981817	47.973287
3503.295503	359925.659208	47.978292
3503.110915	359938.589618	47.983297
3503.139700	359930.137011	47.988301
3503.195081	359934.963069	47.993306
3503.122316	359935.407207	47.998311
3503.410998	359928.363942	48.003316
3503.263138	359932.916776	48.008321
3503.410957	359916.811515	48.013325
3503.395236	359903.938314	48.018330
3503.011939	359902.166838	48.023335
3503.456268	359900.697111	48.028340
3503.167143	359901.837052	48.033345
3503.105081	359901.821469	48.038349
3503.333184	359898.324787	48.043354
3503.186309	359913.361272	48.048359
3503.293632	359903.776615	48.053364
3503.049720	359894.400157	48.058369
3503.214607	359900.964690	48.063373
3503.141601	359905.556586	48.068378
3503.119668	359915.331416	48.073383
3503.618198	359892.249360	48.078388
3503.310901	359884.994950	48.083393
3503.431051	359870.471708	48.088397
3503.238709	359866.787028	48.093402
3503.171465	359865.169157	48.098407
3503.145565	359865.198749	48.103412
3502.657549	359870.823208	48.108417
3502.962479	359868.154102	48.113421
3503.202146	359870.457312	48.118426
3503.180084	359874.125095	48.123431
3503.420277	359869.328748	48.128436
3502.870286	359872.418389	48.133441
3503.512767	359873.258382	48.138445
3503.317036	359874.078206	48.143450
3502.977582	359878.992133	48.148455
3503.065758	359868.163635	48.153460
3503.146669	359858.888498	48.158465
3503.317525	359852.627233	48.163469
3503.506415	359855.600070	48.168474
3503.216543	359859.132068	48.173479
3503.221002	359844.678000	48.178484
3503.194440	359849.491574	48.183489
3503.096946	359852.738700	48.188493
3503.336859	359852.777163	48.193498
3503.372043	359856.690361	48.198503
3503.334201	359860.945901	48.203508
3503.222742	359864.551480	48.208513
3503.411752	359839.609868	48.213517
3503.269791	359826.400356	48.218522
3502.932370	359828.234980	48.223527
3503.478179	359821.125606	48.228532
3503.195768	359826.590336	48.233537
3503.328570	359825.042624	48.238541
3503.583211	359822.305127	48.243546
3503.549895	359824.117123	48.248551
3503.521497	359813.434272	48.253556
3503.213292	359796.841245	48.258561
3503.073604	359787.753645	48.263565
3503.356946	359791.322264	48.268570
3502.958088	359798.001376	48.273575
3503.280217	359791.334496	48.278580
3503.341927	359789.721683	48.283585
3503.209185	359795.951588	48.288589
3503.633919	359795.808158	48.293594
3503.182650	359798.067920	48.298599
3503.269479	359789.911466	48.303604
3503.028883	359774.249252	48.308609
3503.404376	359754.799940	48.313613
3503.415503	359746.630001	48.318618
3503.162832	359751.784683	48.323623
3503.609230	359744.029412	48.328628
3503.579220	359752.176994	48.333633
3503.437279	359760.367716	48.338637
3503.454114	359754.894172	48.343642
3503.467998	359731.201607	48.348647
3503.333051	359725.014114	48.353652
3503.234999	359732.256392	48.358657
3503.079208	359724.876222	48.363661
3503.451077	359718.481378	48.368666
3503.184810	359729.109150	48.373671
3503.171803	359713.385493	48.378676
3503.260420	359717.646501	48.383681
3503.121453	359715.658269	48.388685
3502.963785	359718.685901	48.393690
3502.789492	359721.690713	48.398695
3502.920525	359720.932110	48.403700
3503.000944	359726.899311	48.408705
3503.183423	359719.414773	48.413709
3503.455530	359726.140503	48.418714
3503.255835	359716.578898	48.423719
3503.337785	359692.493860	48.428724
3502.869399	359691.066628	48.433729
3503.086594	359691.490377	48.438733
3503.525543	359688.087580	48.443738
3503.385334	359674.114362	48.448743
3503.456562	359686.444583	48.453748
3503.049750	359695.720483	48.458753
3503.406378	359691.618206	48.463757
3503.303880	359691.100090	48.468762
3502.961316	359695.683726	48.473767
3503.222424	359691.342086	48.478772
3503.116566	359701.588259	48.483777
3503.066177	359683.885695	48.488781
3503.051440	359670.783260	48.493786
3502.885286	359670.911363	48.498791
3503.192134	359678.573120	48.503796
3502.920720	359681.873197	48.508801
3503.126633	359684.894246	48.513805
3503.053240	359681.877797	48.518810
3502.871153	359672.109829	48.523815
3502.986700	359686.621420	48.528820
3503.008741	359695.320601	48.533825
3503.250790	359697.165410	48.538829
3503.205798	359681.370460	48.543834
3503.044040	359667.273415	48.548839
3503.113141	359662.656772	48.553844
3502.911185	359669.126651	48.558849
3502.638442	359669.398835	48.563853
3503.238503	359670.220092	48.568858
3503.200124	359675.290014	48.573863
3503.117832	359666.218764	48.578868
3502.831336	359670.310060	48.583873
3502.906862	359673.606184	48.588877
3503.196394	359677.250171	48.593882
3502.955475	359692.963193	48.598887
3502.902960	359682.894836	48.603892
3503.026117	359696.590941	48.608897
3502.902434	359685.312415	48.613901
3503.308319	359692.296911	48.618906
3502.855178	359696.134640	48.623911
3503.135122	359694.767233	48.628916
3502.909833	359698.772512	48.633921
3503.143508	359703.850316	48.638925
3502.965499	359696.728117	48.643930
3502.815725	359695.988458	48.648935
3503.265077	359705.816059	48.653940
3503.176424	359700.079277	48.658945
3503.338461	359688.272106	48.663949
3503.385784	359690.809300	48.668954
3502.869055	359692.036119	48.673959
3503.243652	359688.439926	48.678964
3502.904888	359694.829644	48.683969
3502.972618	359688.508322	48.688973
3503.415163	359684.697816	48.693978
3503.170935	359689.036891	48.698983
3503.256687	359679.989971	48.703988
3502.994111	359699.523351	48.708993
3503.058790	359685.848548	48.713997
3503.310498	359691.966799	48.719002
3502.874999	359689.872766	48.724007
3502.933497	359693.756844	48.729012
3502.794813	359700.165825	48.734017
3502.854782	359697.408203	48.739021
3503.148714	359691.865402	48.744026
3502.946015	359700.091185	48.749031
3503.396919	359703.785998	48.754036
3503.270541	359697.851609	48.759041
3503.372427	359706.589059	48.764045
3503.554674	359704.499155	48.769050
3503.311169	359693.875729	48.774055
3503.298544	359670.009200	48.779060
3503.161079	359670.158214	48.784065
3503.458328	359666.523354	48.789069
3503.368137	359670.049246	48.794074
3503.077909	359666.558150	48.799079
3503.349631	359660.001006	48.804084
3503.256710	359666.402756	48.809089
3503.106574	359664.950659	48.814093
3503.463857	359668.049565	48.819098
3503.529783	359660.049072	48.824103
3503.391064	359647.602386	48.829108
3503.085330	359637.981189	48.834113
3503.254766	359632.610740	48.839117
3503.165859	359630.411021	48.844122
3502.868211	359637.532188	48.849127
3503.230382	359625.031761	48.854132
3503.176298	359637.509034	48.859137
3503.113638	359634.618117	48.864141
3503.314002	359641.635110	48.869146
3503.318637	359642.041569	48.874151
3503.321429	359630.743037	48.879156
3503.256063	359645.817612	48.884161
3503.503184	359623.589452	48.889165
3503.456109	359600.237260	48.894170
3502.836484	359607.358439	48.899175
3503.359552	359598.776743	48.904180
3503.317939	359599.292299	48.909185
3503.472552	359598.733536	48.914189
3503.430668	359602.811615	48.919194
3502.880815	359602.542342	48.924199
3503.464973	359599.727295	48.929204
3503.310998	359602.830688	48.934209
3503.436987	359583.242626	48.939213
3503.087214	359574.798908	48.944218
3503.028542	359572.797977	48.949223
3503.109940	359562.784764	48.954228
3503.112394	359571.537956	48.959233
3503.121708	359568.635657	48.964237
3503.308773	359562.397238	48.969242
3503.198226	359566.511620	48.974247
3502.947618	359569.172259	48.979252
3502.998887	359579.597188	48.984257
3502.984617	359574.612021	48.989261
3503.152116	359570.285169	48.994266
3502.830641	359576.952079	48.999271
3503.291451	359576.981069	49.004276
3502.936536	359579.480072	49.009281
3502.977663	359577.539703	49.014285
3503.195987	359583.815923	49.019290
3503.240877	359578.694173	49.024295
3503.276631	359573.548420	49.029300
3503.304777	359579.931043	49.034305
3503.197185	359577.047225	49.039309
3503.199015	359573.509952	49.044314
3503.227416	359587.068390	49.049319
3503.463646	359549.828603	49.054324
3503.677787	359551.728722	49.059329
3503.492741	359541.401377	49.064333
3503.513176	359540.558469	49.069338
3503.556646	359536.327560	49.074343
3503.779593	359524.256257	49.079348
3503.143826	359517.384519	49.084353
3503.341901	359503.917594	49.089357
3503.425625	359497.313809	49.094362
3503.075145	359503.807190	49.099367
3503.392297	359502.790144	49.104372
3503.243228	359509.175345	49.109377
3503.417686	359501.870166	49.114381
3503.173637	359479.465122	49.119386
3503.227067	359468.336671	49.124391
3503.350641	359459.970783	49.129396
3503.234949	359467.470353	49.134401
3503.076222	359463.907560	49.139405
3503.467599	359467.662695	49.144410
3502.959138	359472.119899	49.149415
3503.421229	359461.384878	49.154420
3503.399720	359469.887413	49.159425
3503.203175	359462.488200	49.164429
3503.028119	359470.429742	49.169434
3503.189307	359475.035548	49.174439
3503.317336	359467.483240	49.179444
3502.921519	359453.168671	49.184449
3502.968363	359438.784120	49.189453
3503.436157	359445.249938	49.194458
3503.102186	359440.595207	49.199463
3503.046517	359442.868786	49.204468
3503.073415	359441.057893	49.209473
3502.984177	359433.056445	49.214477
3503.191631	359450.759820	49.219482
3503.323528	359447.430994	49.224487
3503.242497	359438.970214	49.229492
3502.938307	359446.550479	49.234497
3503.221309	359443.070533	49.239501
3503.415906	359448.739808	49.244506
3503.121707	359444.333254	49.249511
3503.143475	359437.688362	49.254516
3503.230788	359448.336639	49.259521
3503.143434	359442.523282	49.264525
3503.232988	359448.514519	49.269530
3503.023518	359453.764189	49.274535
3503.266183	359436.396903	49.279540
3503.105752	359436.676780	49.284545
3503.019375	359426.232027	49.289549
3503.309187	359411.172899	49.294554
3503.251479	359403.929853	49.299559
3503.098061	359400.518895	49.304564
3503.124403	359405.222364	49.309569
3503.020479	359401.192869	49.314573
3502.828511	359404.505852	49.319578
3502.589457	359409.200383	49.324583
3503.293397	359403.898090	49.329588
3502.960311	359412.398997	49.334593
3502.975570	359414.356008	49.339597
3503.224708	359407.980525	49.344602
3502.818945	359411.887126	49.349607
3503.035628	359406.152933	49.354612
3503.117424	359418.227087	49.359617
3503.254368	359414.184961	49.364621
3503.040381	359412.412148	49.369626
3503.146928	359407.153400	49.374631
3503.538782	359414.598190	49.379636
3503.259381	359420.545971	49.384641
3503.078806	359416.681272	49.389645
3503.426665	359409.475899	49.394650
3503.275918	359412.731472	49.399655
3503.284543	359416.547118	49.404660
3503.108734	359430.672256	49.409665
3502.828836	359425.398263	49.414669
3503.098679	359421.055218	49.419674
3502.894781	359424.166515	49.424679
3503.303524	359415.475628	49.429684
3503.042844	359429.614183	49.434689
3503.098498	359419.528671	49.439693
3503.454566	359414.383157	49.444698
3503.049404	359401.622280	49.449703
3502.938736	359398.357242	49.454708
3503.055960	359399.611082	49.459713
3503.225185	359398.973668	49.464717
3503.349760	359401.066077	49.469722
3503.156986	359405.600614	49.474727
3503.475864	359402.598475	49.479732
3503.384087	359401.595180	49.484737
3503.335430	359408.371663	49.489741
3503.238088	359405.715232	49.494746
3503.256415	359401.132036	49.499751
3503.272486	359403.750525	49.504756
3503.344863	359380.303005	49.509761
3503.288893	359369.166380	49.514765
3503.096807	359364.463765	49.519770
3502.647820	359377.766926	49.524775
3503.000392	359359.008132	49.529780
3502.918427	359364.568459	49.534785
3503.039863	359368.264489	49.539789
3503.244874	359366.349097	49.544794
3503.316132	359365.396367	49.549799
3503.102013	359366.346338	49.554804
3503.207910	359372.156876	49.559809
3503.349512	359371.142133	49.564813
3503.096249	359367.110797	49.569818
3502.989254	359372.776865	49.574823
3502.966957	359376.800973	49.579828
3502.988448	359369.316384	49.584833
3502.979477	359382.142842	49.589837
3503.083398	359368.258175	49.594842
3503.234537	359380.524947	49.599847
3503.301055	359370.997528	49.604852
3503.219637	359371.315808	49.609857
3503.229874	359380.882089	49.614861
3503.053125	359371.851162	49.619866
3502.910936	359377.268330	49.624871
3503.271567	359379.705119	49.629876
3503.045962	359381.038601	49.634881
3503.048546	359382.030654	49.639885
3503.072853	359376.581333	49.644890
3502.942386	359386.297088	49.649895
3503.276824	359372.325089	49.654900
3502.942841	359391.640863	49.659905
3503.073432	359389.660898	49.664909
3503.227596	359383.478550	49.669914
3502.787624	359375.557985	49.674919
3502.993747	359387.714277	49.679924
3503.172551	359393.360609	49.684929
3503.442957	359386.905422	49.689933
3503.302164	359362.473736	49.694938
3502.902097	359362.791496	49.699943
3503.483283	359350.612625	49.704948
3503.238845	359356.529441	49.709953
3503.182516	359357.912503	49.714957
3503.650154	359354.530595	49.719962
3503.281003	359352.756862	49.724967
3503.199445	359359.589445	49.729972
3502.946003	359365.914826	49.734977
3503.032777	359358.470808	49.739981
3503.113123	359362.656816	49.744986
3503.034645	359358.521508	49.749991
3503.111402	359361.842906	49.754996
3503.065217	359361.723027	49.760001
3502.987632	359361.277308	49.765005
3503.267810	359351.359859	49.770010
3502.967544	359340.389079	49.775015
3502.925542	359325.738629	49.780020
3502.980187	359339.242094	49.785025
3503.298604	359348.912342	49.790029
3503.327422	359337.889538	49.795034
3503.065897	359335.030040	49.800039
3503.082001	359321.210135	49.805044
3502.961431	359323.493979	49.810049
3503.008611	359324.987912	49.815053
3503.100847	359322.505079	49.820058
3502.662367	359331.862394	49.825063
3502.860943	359337.174803	49.830068
3502.863376	359346.589646	49.835073
3502.807542	359362.349855	49.840077
3503.127103	359364.615013	49.845082
3502.910660	359375.387664	49.850087
3503.306176	359363.416272	49.855092
3503.074834	359377.855562	49.860097
3503.235989	359368.643985	49.865101
3503.336863	359346.769621	49.870106
3503.038536	359339.793621	49.875111
3503.154014	359327.306669	49.880116
3503.181730	359338.753231	49.885121
3503.231053	359340.781199	49.890125
3503.192087	359330.354377	49.895130
3502.725322	359341.599197	49.900135
3502.946178	359336.475050	49.905140
3502.873240	359343.484399	49.910145
3502.732153	359342.819701	49.915149
3503.202730	359345.697146	49.920154
3502.926282	359339.608312	49.925159
3502.891008	359351.319293	49.930164
3502.838156	359347.434398	49.935169
3502.767956	359366.683036	49.940173
3503.090198	359376.861602	49.945178
3502.978293	359388.075760	49.950183
3503.187436	359388.093642	49.955188
3503.268023	359385.612654	49.960193
3502.955677	359363.320139	49.965197
3503.325249	359345.907312	49.970202
3503.204443	359354.221994	49.975207
3502.935781	359348.310055	49.980212
3503.078146	359353.071527	49.985217
3502.893857	359357.986424	49.990221
3503.388157	359351.394052	49.995226
3503.103501	359362.152044	50.000231
3503.259552	359346.808684	50.005236
3503.048053	359354.501542	50.010241
3502.906084	359353.913323	50.015245
3503.250175	359358.719244	50.020250
3503.151154	359358.607718	50.025255
3503.263155	359359.582474	50.030260
3503.152771	359361.559349	50.035265
3503.151590	359355.019859	50.040269
3503.228069	359365.695314	50.045274
3502.900719	359353.532837	50.050279
3503.182635	359356.109302	50.055284
3502.919865	359350.094647	50.060289
3503.401489	359364.599356	50.065293
3503.418943	359361.339508	50.070298
3503.108256	359345.357433	50.075303
3503.178957	359340.206131	50.080308
3503.079711	359344.216960	50.085313
3503.548388	359326.025066	50.090317
3503.518531	359322.594570	50.095322
3502.968727	359333.598055	50.100327
3503.423805	359334.747594	50.105332
3503.204546	359327.097486	50.110337
3503.316971	359326.799854	50.115341
3503.220343	359332.515181	50.120346
3503.244205	359334.674407	50.125351
3503.308425	359319.803592	50.130356
3503.417712	359312.915830	50.135361
3503.302376	359302.857324	50.140365
3503.330296	359296.974833	50.145370
3503.159191	359312.168013	50.150375
3503.313005	359295.170973	50.155380
3503.242756	359308.821423	50.160385
3503.182329	359308.220312	50.165389
3503.264590	359301.311374	50.170394
3502.940693	359312.279152	50.175399
3503.287627	359295.760511	50.180404
3503.124447	359310.290831	50.185409
3503.657926	359289.086000	50.190413
3503.588089	359270.597519	50.195418
3503.243935	359271.288138	50.200423
3503.340530	359255.267094	50.205428
3503.382237	359270.095841	50.210433
3503.194733	359275.469290	50.215437
3503.331717	359267.584731	50.220442
3503.103670	359276.399861	50.225447
3503.384186	359260.298851	50.230452
3503.142204	359259.344745	50.235457
3503.275504	359238.762976	50.240461
3503.445492	359235.708024	50.245466
3502.972628	359237.284170	50.250471
3503.061125	359228.491197	50.255476
3503.099516	359235.737426	50.260481
3503.162581	359238.373942	50.265485
3503.367465	359227.196047	50.270490
3503.370537	359235.643844	50.275495
3503.558092	359236.224962	50.280500
3503.203862	359238.316730	50.285505
3503.218071	359226.736387	50.290509
3503.525304	359198.518607	50.295514
3502.837979	359187.201835	50.300519
3503.179375	359205.545736	50.305524
3503.664169	359191.295450	50.310529
3503.250967	359195.126904	50.315533
3503.021767	359199.387308	50.320538
3503.226919	359201.670559	50.325543
3503.473458	359192.928935	50.330548
3503.414487	359204.618251	50.335553
3503.412384	359193.803874	50.340557
3503.545037	359164.748491	50.345562
3503.017891	359157.808638	50.350567
3503.217300	359149.252582	50.355572
3503.248619	359164.693719	50.360577
3503.407008	359161.564257	50.365581
3503.407852	359161.411496	50.370586
3503.267175	359150.669909	50.375591
3503.407270	359153.828629	50.380596
3503.287557	359154.814574	50.385601
3503.056431	359139.303337	50.390605
3503.563139	359122.733933	50.395610
3503.400566	359116.805195	50.400615
3503.353753	359121.418471	50.405620
3503.392952	359121.768577	50.410625
3503.255153	359116.751998	50.415629
3503.748581	359122.195946	50.420634
3503.208683	359113.146039	50.425639
3503.101702	359094.841490	50.430644
3503.423938	359086.749490	50.435649
3503.097694	359092.450251	50.440653
3503.255802	359083.442674	50.445658
3503.405165	359081.383390	50.450663
3503.538976	359089.021701	50.455668
3503.251826	359088.430983	50.460673
3502.695623	359090.223881	50.465677
3502.832294	359079.031289	50.470682
3502.697165	359094.549654	50.475687
3503.132723	359087.457602	50.480692
3503.081782	359089.501431	50.485697
3503.001395	359092.669563	50.490701
3503.157636	359087.123014	50.495706
3502.870008	359094.191783	50.500711
3502.994832	359082.670260	50.505716
3503.391163	359087.111698	50.510721
3503.164543	359083.050680	50.515725
3503.555441	359080.596960	50.520730
3503.111033	359068.681935	50.525735
3503.143948	359032.542649	50.530740
3503.205682	359021.438230	50.535745
3502.813214	358971.166945	50.540749
3502.879774	358930.060174	50.545754
3502.447194	358875.647331	50.550759
3502.284449	358808.213954	50.555764
3501.897679	358751.834335	50.560769
3501.658094	358674.768611	50.565773
3501.431570	358576.656184	50.570778
3501.034585	358498.571746	50.575783
3500.988936	358391.752976	50.580788
3500.755321	358305.015897	50.585793
3500.147472	358187.801411	50.590797
3499.846390	358080.386170	50.595802
3499.531677	357954.549122	50.600807
3499.190916	357829.733760	50.605812
3498.791719	357712.154345	50.610817
3498.628556	357581.075700	50.615821
3498.338133	357437.980204	50.620826
3497.182139	357299.194519	50.625831
3497.166485	357143.152865	50.630836
3496.492687	357005.511616	50.635841
3496.032522	356854.272590	50.640845
3495.760269	356710.128778	50.645850
3495.389116	356545.667351	50.650855
3494.761320	356386.869953	50.655860
3494.181581	356215.136860	50.660865
3493.733181	356052.391052	50.665869
3493.235651	355864.509666	50.670874
3492.475322	355709.904598	50.675879
3492.150131	355531.283356	50.680884
3491.894981	355344.226973	50.685889
3491.147597	355159.309056	50.690893
3490.505024	354986.385660	50.695898
3489.785852	354799.069808	50.700903
3489.089505	354608.059585	50.705908
3488.451349	354425.310353	50.710913
3487.862120	354242.171004	50.715917
3487.707985	354055.221205	50.720922
3486.541725	353886.143376	50.725927
3486.161724	353679.682954	50.730932
3485.603752	353492.056943	50.735937
3484.909532	353301.016120	50.740941
3484.394802	353109.640829	50.745946
3483.703160	352914.704407	50.750951
3483.360351	352712.408035	50.755956
3482.260293	352516.822116	50.760961
3482.038331	352331.200279	50.765965
3481.318982	352126.594351	50.770970
3480.329026	351941.296166	50.775975
3480.093437	351732.845627	50.780980
3479.521365	351531.344508	50.785985
3478.528746	351333.090420	50.790989
3478.053086	351131.088998	50.795994
3477.475059	350926.023480	50.800999
3476.901416	350714.950123	50.806004
3476.116236	350533.890427	50.811009
3475.550257	350322.559824	50.816013
3474.860483	350113.538561	50.821018
3473.886336	349918.864963	50.826023
3473.248855	349706.245274	50.831028
3472.775982	349512.661738	50.836033
3471.875358	349302.398154	50.841037
3471.084435	349099.217382	50.846042
3470.774001	348903.391753	50.851047
3470.324702	348704.355029	50.856052
3469.416430	348501.928721	50.861057
3468.557114	348296.541527	50.866061
3468.249743	348094.196903	50.871066
3467.079588	347892.878776	50.876071
3466.508179	347686.069421	50.881076
3466.025815	347494.312928	50.886081
3465.455372	347291.090734	50.891085
3464.690064	347086.346026	50.896090
3464.094029	346895.445409	50.901095
3463.256702	346674.446487	50.906100
3462.780401	346479.198615	50.911105
3462.226197	346270.930599	50.916109
3461.633071	346064.933284	50.921114
3460.773356	345864.653382	50.926119
3459.933401	345665.947749	50.931124
3459.324854	345451.831185	50.936129
3458.570023	345234.428047	50.941133
3458.073366	345047.374492	50.946138
3457.616836	344842.369381	50.951143
3456.645932	344629.147056	50.956148
3455.855342	344431.931180	50.961153
3454.704931	344233.651577	50.966157
3454.516772	344039.139043	50.971162
3453.474623	343829.946788	50.976167
3453.025813	343630.917902	50.981172
3452.535373	343438.894775	50.986177
3451.753526	343239.815429	50.991181
3450.923055	343036.924993	50.996186
3449.829854	342843.391655	51.001191
3449.753063	342640.813448	51.006196
3449.000231	342451.984998	51.011201
3448.152277	342247.261967	51.016205
3447.899585	342049.749587	51.021210
3447.102346	341851.991758	51.026215
3446.382721	341652.566464	51.031220
3445.689682	341460.747303	51.036225
3445.083572	341264.484655	51.041229
3444.481498	341059.591519	51.046234
3443.590487	340859.681669	51.051239
3443.323441	340656.847004	51.056244
3442.567226	340461.241935	51.061249
3441.533844	340262.243617	51.066253
3441.080971	340060.632804	51.071258
3440.288712	339864.853391	51.076263
3439.747128	339660.327953	51.081268
3438.910857	339463.841507	51.086273
3438.236011	339265.317933	51.091277
3437.864262	339057.989039	51.096282
3436.863993	338871.250800	51.101287
3436.448053	338654.661668	51.106292
3435.568463	338458.331725	51.111297
3434.767662	338267.996361	51.116301
3434.328718	338070.526416	51.121306
3433.750963	337875.496162	51.126311
3432.938699	337672.941884	51.131316
3432.000161	337481.556839	51.136321
3431.292872	337286.901704	51.141325
3431.045763	337084.154426	51.146330
3429.899394	336905.325181	51.151335
3429.583668	336697.572620	51.156340
3428.926223	336503.009128	51.161345
3428.410929	336306.615158	51.166349
3427.680920	336103.584854	51.171354
3427.128782	335916.410966	51.176359
3426.254632	335706.910729	51.181364
3425.556468	335514.234636	51.186369
3424.738177	335319.642243	51.191373
3424.290658	335116.335196	51.196378
3423.308011	334929.532146	51.201383
3422.942346	334735.121094	51.206388
3422.195763	334532.063261	51.211393
3421.183096	334338.491660	51.216397
3420.706165	334151.428335	51.221402
3420.126647	333966.111850	51.226407
3419.493857	333760.106130	51.231412
3418.806839	333563.833274	51.236417
3417.927403	333364.331682	51.241421
3417.722835	333173.403987	51.246426
3416.639531	332987.400837	51.251431
3416.006574	332779.788418	51.256436
3415.606312	332588.711885	51.261441
3414.934279	332396.226693	51.266445
3414.401403	332187.527479	51.271450
3413.382962	332005.330264	51.276455
3412.961327	331801.933149	51.281460
3412.164613	331606.283250	51.286465
3411.291046	331414.972941	51.291469
3410.763953	331219.584873	51.296474
3409.863174	331028.583358	51.301479
3409.365320	330833.622435	51.306484
3408.642196	330638.620241	51.311489
3407.985167	330447.400464	51.316493
3407.551563	330252.096882	51.321498
3406.319770	330067.637271	51.326503
3405.950990	329867.968931	51.331508
3405.476535	329680.409892	51.336513
3404.752577	329487.339718	51.341517
3404.238447	329288.736654	51.346522
3403.245961	329096.318966	51.351527
3402.379215	328910.525830	51.356532
3401.865604	328715.561889	51.361537
3401.261045	328534.334554	51.366541
3400.688811	328336.883882	51.371546
3400.018871	328147.035149	51.376551
3399.514006	327956.472435	51.381556
3398.677310	327764.866951	51.386561
3398.063384	327568.261089	51.391565
3397.440964	327366.895061	51.396570
3396.406851	327196.705778	51.401575
3395.653663	326998.261928	51.406580
3395.234825	326809.006745	51.411585
3394.437588	326621.898685	51.416589
3393.782137	326422.750517	51.421594
3393.275885	326245.041322	51.426599
3392.929877	326044.952171	51.431604
3391.992385	325863.822252	51.436609
3391.196797	325677.399163	51.441613
3390.643630	325479.480055	51.446618
3389.827430	325291.557167	51.451623
3388.920006	325098.912585	51.456628
3388.562929	324912.469329	51.461633
3387.386333	324729.694296	51.466637
3387.020628	324529.884617	51.471642
3386.120676	324356.180004	51.476647
3385.521287	324176.698781	51.481652
3384.932117	323996.222577	51.486657
3384.360741	323810.829182	51.491661
3384.018994	323610.631604	51.496666
3383.138808	323435.979901	51.501671
3382.414201	323244.116891	51.506676
3381.770206	323046.613752	51.511681
3381.246275	322866.812285	51.516685
3380.523776	322684.368393	51.521690
3379.707130	322492.823796	51.526695
3379.273243	322305.062938	51.531700
3378.510443	322127.029092	51.536705
3377.700226	321938.359417	51.541709
3377.123303	321741.912088	51.546714
3376.467593	321564.725864	51.551719
3375.920065	321366.567114	51.556724
3374.899508	321183.683456	51.561729
3374.228296	321004.818084	51.566733
3373.754386	320814.768814	51.571738
3373.112486	320634.319426	51.576743
3372.717088	320448.101732	51.581748
3372.071943	320257.467279	51.586753
3371.163268	320070.082335	51.591757
3370.594348	319871.007041	51.596762
3369.716545	319699.199337	51.601767
3369.331525	319507.350922	51.606772
3368.391672	319317.499530	51.611777
3367.886041	319136.516395	51.616781
3367.352602	318948.560587	51.621786
3366.505919	318761.748828	51.626791
3366.014321	318563.295070	51.631796
3365.244217	318369.391826	51.636801
3364.357193	318202.802673	51.641805
3363.836050	318011.354672	51.646810
3363.203446	317832.018734	51.651815
3362.774456	317637.576269	51.656820
3361.591010	317448.574467	51.661825
3361.200376	317263.393673	51.666829
3360.668893	317067.489425	51.671834
3359.976255	316885.334843	51.676839
3359.303777	316699.713758	51.681844
3358.567073	316505.012147	51.686849
3357.468872	316326.052637	51.691853
3357.125130	316134.063641	51.696858
3356.478291	315956.839978	51.701863
3356.125820	315768.009108	51.706868
3355.365228	315576.797945	51.711873
3354.509121	315393.698891	51.716877
3354.050764	315199.740103	51.721882
3353.283843	315021.286090	51.726887
3352.700152	314822.075466	51.731892
3351.922541	314634.022718	51.736897
3351.064147	314458.204952	51.741901
3350.769224	314262.792598	51.746906
3349.945722	314078.820299	51.751911
3349.006774	313883.432702	51.756916
3348.365405	313706.178851	51.761921
3347.620148	313523.288157	51.766925
3347.513881	313331.001771	51.771930
3346.364022	313153.038040	51.776935
3346.007287	312968.837227	51.781940
3345.287809	312781.535929	51.786945
3344.297691	312593.233085	51.791949
3343.583796	312403.154673	51.796954
3343.064599	312226.541149	51.801959
3342.480954	312040.566709	51.806964
3342.092897	311864.186511	51.811969
3341.002161	311677.298558	51.816973
3340.741501	311492.341627	51.821978
3339.753680	311306.913716	51.826983
3339.408047	311112.853360	51.831988
3338.712790	310928.575391	51.836993
3337.822531	310749.573654	51.841997
3337.409129	310555.599468	51.847002
3336.557113	310373.433498	51.852007
3336.048176	310183.217095	51.857012
3335.156071	309993.824923	51.862017
3334.266079	309820.754985	51.867021
3333.892911	309626.900225	51.872026
3332.893909	309444.654210	51.877031
3332.249947	309269.583774	51.882036
3331.637661	309099.397325	51.887041
3331.260034	308916.721195	51.892045
3330.558502	308723.146099	51.897050
3329.706831	308548.718634	51.902055
3328.947574	308362.053105	51.907060
3328.409757	308176.625524	51.912065
3327.768418	307990.068111	51.917069
3326.795568	307813.596108	51.922074
3325.941137	307645.279442	51.927079
3325.430055	307455.874006	51.932084
3324.891222	307273.271892	51.937089
3324.102767	307104.460238	51.942093
3323.566187	306930.413607	51.947098
3322.951193	306753.705284	51.952103
3322.357921	306570.525085	51.957108
3321.461547	306384.616840	51.962113
3320.985684	306213.004328	51.967117
3320.564525	306035.296696	51.972122
3319.805131	305848.933122	51.977127
3319.248042	305669.489384	51.982132
3318.584458	305480.843714	51.987137
3317.779915	305307.524904	51.992141
3317.392410	305122.272929	51.997146
3316.470049	304943.700906	52.002151
3315.521670	304761.134653	52.007156
3315.119517	304584.873667	52.012161
3314.368307	304402.530417	52.017165
3313.693139	304222.670553	52.022170
3313.013069	304047.726141	52.027175
3312.312322	303858.804026	52.032180
3311.443723	303682.539295	52.037185
3310.716020	303499.860116	52.042189
3310.092849	303322.435629	52.047194
3309.609671	303147.509917	52.052199
3309.172149	302980.191117	52.057204
3308.520130	302795.512741	52.062209
3307.552997	302612.513807	52.067213
3307.058152	302435.144358	52.072218
3306.459710	302259.930243	52.077223
3305.395436	302075.621784	52.082228
3304.894580	301894.789256	52.087233
3304.521936	301709.123120	52.092237
3304.076105	301536.176002	52.097242
3303.024142	301352.756053	52.102247
3302.473173	301178.017064	52.107252
3301.971155	301007.777682	52.112257
3301.168551	300829.181759	52.117261
3300.678406	300630.264957	52.122266
3299.688314	300455.721967	52.127271
3299.059218	300277.301723	52.132276
3298.777532	300102.366177	52.137281
3297.859268	299925.366479	52.142285
3297.190772	299736.179546	52.147290
3296.297102	299560.321567	52.152295
3295.738120	299375.751823	52.157300
3295.033563	299191.510505	52.162305
3294.049603	299020.963309	52.167309
3293.805207	298834.229492	52.172314
3293.112931	298668.525416	52.177319
3292.294033	298487.026373	52.182324
3291.630269	298315.893041	52.187329
3290.878270	298140.647884	52.192333
3290.757736	297969.504698	52.197338
3289.521838	297791.865462	52.202343
3289.178506	297607.183355	52.207348
3288.382188	297424.864733	52.212353
3287.177316	297249.333816	52.217357
3287.014204	297076.643053	52.222362
3286.071154	296898.956640	52.227367
3285.638782	296732.165551	52.232372
3285.014907	296559.801868	52.237377
3284.187660	296382.860670	52.242381
3283.805703	296200.730001	52.247386
3282.910553	296021.609051	52.252391
3282.331804	295848.218921	52.257396
3282.141295	295666.719623	52.262401
3281.218746	295492.008342	52.267405
3280.496366	295313.521577	52.272410
3279.604207	295131.165034	52.277415
3279.156622	294965.444492	52.282420
3278.164916	294785.446374	52.287425
3277.739321	294610.324668	52.292429
3277.363402	294424.116701	52.297434
3276.530200	294266.351459	52.302439
3275.748692	294081.862725	52.307444
3275.140425	293892.227501	52.312449
3274.184019	293727.375974	52.317453
3273.770052	293545.986606	52.322458
3272.980512	293373.697422	52.327463
3272.225229	293203.618352	52.332468
3271.663330	293034.985677	52.337473
3270.814648	292850.404690	52.342477
3270.637879	292676.439074	52.347482
3269.487143	292505.352415	52.352487
3269.122994	292339.107371	52.357492
3268.572022	292153.943933	52.362497
3267.778905	291982.723932	52.367501
3266.930498	291807.208541	52.372506
3266.183389	291621.031559	52.377511
3265.538188	291445.916720	52.382516
3265.152446	291287.874950	52.387521
3264.346951	291109.652721	52.392525
3264.088894	290916.063191	52.397530
3263.115527	290750.626561	52.402535
3262.531923	290579.092334	52.407540
3261.836997	290403.857326	52.412545
3261.138905	290228.393496	52.417549
3260.753999	290057.158590	52.422554
3259.479759	289876.437454	52.427559
3258.929437	289707.979017	52.432564
3258.433638	289521.709886	52.437569
3257.653654	289358.381127	52.442573
3257.084646	289174.211712	52.447578
3256.375977	289008.528441	52.452583
3255.875933	288835.630149	52.457588
3255.287391	288657.168301	52.462593
3254.673547	288473.642247	52.467597
3253.996872	288307.316840	52.472602
3253.103640	288125.642998	52.477607
3252.577307	287952.340890	52.482612
3251.764646	287778.192606	52.487617
3251.047972	287602.042548	52.492621
3250.582375	287419.765842	52.497626
3249.827425	287250.039576	52.502631
3248.871737	287086.304486	52.507636
3248.215112	286896.570139	52.512641
3247.042507	286731.901416	52.517645
3246.761953	286556.751493	52.522650
3246.260556	286401.068517	52.527655
3245.375391	286231.795324	52.532660
3244.620044	286068.384635	52.537665
3244.176795	285905.128249	52.542669
3243.830421	285719.011621	52.547674
3242.827719	285554.875805	52.552679
3242.044919	285391.571049	52.557684
3241.666799	285215.824719	52.562689
3241.028575	285056.775599	52.567693
3240.533865	284874.018373	52.572698
3239.633832	284710.986580	52.577703
3239.207967	284532.114942	52.582708
3238.766973	284366.107037	52.587713
3237.647576	284186.377186	52.592717
3237.123583	284002.096147	52.597722
3236.371733	283848.565696	52.602727
3235.525608	283662.399906	52.607732
3235.373813	283499.147448	52.612737
3234.378256	283324.924283	52.617741
3233.531705	283150.117186	52.622746
3233.042661	282983.989073	52.627751
3232.735072	282812.127320	52.632756
3231.863298	282628.384700	52.637761
3231.176026	282471.405417	52.642765
3230.386640	282282.352258	52.647770
3229.531693	282122.827115	52.652775
3228.861928	281967.016468	52.657780
3228.377119	281786.956204	52.662785
3227.574930	281622.991109	52.667789
3226.914100	281456.176631	52.672794
3225.905659	281292.778917	52.677799
3225.383332	281119.269756	52.682804
3224.883942	280953.779437	52.687809
3223.787970	280797.246430	52.692813
3223.175327	280620.975394	52.697818
3222.737026	280462.937518	52.702823
3222.104224	280304.013522	52.707828
3221.375170	280134.331622	52.712833
3220.941450	279977.540877	52.717837
3220.354866	279796.401094	52.722842
3219.560524	279646.416451	52.727847
3218.925011	279469.613963	52.732852
3218.527810	279305.304168	52.737857
3217.384661	279144.244966	52.742861
3217.191152	278967.525277	52.747866
3216.533987	278802.798104	52.752871
3215.542937	278633.310210	52.757876
3214.798442	278460.676147	52.762881
3214.023410	278299.100164	52.767885
3213.619675	278134.027192	52.772890
3212.763531	277969.586079	52.777895
3212.218458	277799.823782	52.782900
3211.446801	277633.790230	52.787905
3210.534035	277475.928869	52.792909
3210.404675	277318.376518	52.797914
3209.826678	277150.096538	52.802919
3209.031699	276979.176694	52.807924
3208.475445	276810.664035	52.812929
3207.671826	276639.643663	52.817933
3207.412360	276471.084032	52.822938
3206.279861	276305.998873	52.827943
3205.539566	276140.928064	52.832948
3204.983012	275976.668637	52.837953
3204.416662	275802.732767	52.842957
3203.848135	275641.531435	52.847962
3202.975783	275470.318155	52.852967
3202.406155	275302.622555	52.857972
3201.602611	275137.841892	52.862977
3201.064060	274973.375863	52.867981
3200.301295	274807.187992	52.872986
3199.315029	274650.153169	52.877991
3198.983775	274478.472269	52.882996
3198.504898	274314.786338	52.888001
3197.383180	274159.275598	52.893005
3197.147127	273991.756474	52.898010
3196.289053	273818.478042	52.903015
3195.675126	273655.704906	52.908020
3194.902073	273491.326981	52.913025
3193.918459	273332.228868	52.918029
3193.396771	273166.792464	52.923034
3192.849012	273012.566285	52.928039
3191.946540	272850.017146	52.933044
3191.628813	272681.772468	52.938049
3190.798369	272528.940884	52.943053
3190.289229	272359.605918	52.948058
3189.782343	272205.093204	52.953063
3189.053612	272027.694085	52.958068
3188.256578	271873.940431	52.963073
3187.462550	271710.610222	52.968077
3187.188266	271548.242008	52.973082
3186.147058	271389.739005	52.978087
3185.369367	271229.971854	52.983092
3185.247534	271051.025179	52.988097
3184.181092	270896.830397	52.993101
3183.748836	270736.168221	52.998106
3183.041310	270570.710646	53.003111
3182.497767	270400.744735	53.008116
3181.636921	270238.749707	53.013121
3180.716468	270079.056291	53.018125
3180.481900	269921.928560	53.023130
3179.805122	269760.210130	53.028135
3178.747155	269588.848629	53.033140
3178.486258	269434.526681	53.038145
3177.395702	269271.065583	53.043149
3177.072514	269110.539306	53.048154
3176.394460	268947.013022	53.053159
3175.705025	268779.362725	53.058164
3175.200941	268609.391004	53.063169
3174.074783	268455.282598	53.068173
3173.824775	268282.596605	53.073178
3172.886343	268132.635374	53.078183
3172.335771	267967.739374	53.083188
3171.861581	267799.647811	53.088193
3171.308362	267636.254954	53.093197
3170.491335	267480.289667	53.098202
3169.517055	267323.075898	53.103207
3168.935512	267146.036729	53.108212
3168.427998	266983.197150	53.113217
3167.597132	266833.142870	53.118221
3167.025902	266658.725468	53.123226
3166.523227	266499.883790	53.128231
3165.682694	266332.436457	53.133236
3164.852388	266175.276692	53.138241
3164.128102	266009.619324	53.143245
3163.972136	265857.930493	53.148250
3163.233906	265693.294178	53.153255
3162.387402	265526.128249	53.158260
3161.530393	265361.689135	53.163265
3160.571368	265211.018988	53.168269
3160.574112	265041.401290	53.173274
3159.778911	264900.255862	53.178279
3159.108872	264735.430871	53.183284
3158.542108	264568.144679	53.188289
3157.436350	264408.507846	53.193293
3156.995955	264244.003287	53.198298
3156.232417	264088.234517	53.203303
3155.786474	263920.827630	53.208308
3155.182458	263754.693763	53.213313
3154.187999	263606.245583	53.218317
3153.562848	263455.803468	53.223322
3153.169193	263296.563819	53.228327
3152.333129	263128.149390	53.233332
3151.606414	262970.694414	53.238337
3150.963502	262816.384273	53.243341
3150.394045	262654.498620	53.248346
3149.757367	262493.897079	53.253351
3148.906002	262332.361811	53.258356
3148.197880	262182.595576	53.263361
3147.434646	262025.197782	53.268365
3147.254309	261860.831525	53.273370
3146.404488	261718.982963	53.278375
3145.558570	261544.203990	53.283380
3145.073647	261381.872679	53.288385
3144.385974	261220.643187	53.293389
3143.905663	261067.046768	53.298394
3143.201207	260909.258254	53.303399
3142.455933	260741.671213	53.308404
3141.858500	260584.528107	53.313409
3140.942235	260431.535841	53.318413
3140.289072	260272.109641	53.323418
3139.833210	260116.064983	53.328423
3139.339228	259948.642407	53.333428
3138.468669	259779.853338	53.338433
3137.581203	259634.802874	53.343437
3137.090524	259470.563534	53.348442
3136.280974	259316.205245	53.353447
3135.582088	259145.020941	53.358452
3135.308572	258989.890407	53.363457
3134.405495	258845.275814	53.368461
3133.864617	258679.185804	53.373466
3133.109516	258519.038266	53.378471
3132.529170	258364.364160	53.383476
3131.597065	258201.545288	53.388481
3130.926721	258035.552611	53.393485
3130.610701	257876.965942	53.398490
3129.374209	257733.550815	53.403495
3128.964410	257575.030127	53.408500
3128.431440	257408.939757	53.413505
3127.475389	257259.826791	53.418509
3126.721194	257107.167487	53.423514
3126.294366	256956.239198	53.428519
3125.480371	256798.674373	53.433524
3125.032319	256646.603626	53.438529
3124.285903	256490.352629	53.443533
3123.709038	256335.501082	53.448538
3122.572107	256185.882657	53.453543
3122.103048	256023.552374	53.458548
3121.580698	255872.843696	53.463553
3120.815405	255726.375656	53.468557
3120.254577	255566.734305	53.473562
3119.556893	255415.875434	53.478567
3118.819236	255267.773450	53.483572
3118.252815	255115.366002	53.488577
3117.583107	254961.727127	53.493581
3116.834036	254801.403088	53.498586
3116.114451	254654.852189	53.503591
3115.851477	254505.198565	53.508596
3115.035330	254349.749712	53.513601
3114.277579	254199.461543	53.518605
3113.741463	254038.875228	53.523610
3112.883400	253889.774657	53.528615
3112.396892	253739.494860	53.533620
3111.891087	253583.895652	53.538625
3111.034868	253424.481058	53.543629
3110.357699	253255.819261	53.548634
3109.796462	253113.217322	53.553639
3108.881071	252960.535741	53.558644
3108.358697	252804.303142	53.563649
3107.439115	252657.989180	53.568653
3107.099427	252501.447799	53.573658
3106.487334	252349.839277	53.578663
3105.807959	252195.873128	53.583668
3105.195863	252049.307275	53.588673
3104.149905	251893.438467	53.593677
3103.672468	251730.731168	53.598682
3103.084019	251588.567692	53.603687
3102.294459	251436.325917	53.608692
3101.854891	251280.972902	53.613697
3101.020492	251131.336088	53.618701
3100.195440	250970.059720	53.623706
3099.943403	250820.865821	53.628711
3099.178143	250663.884129	53.633716
3098.461518	250509.874465	53.638721
3097.645268	250364.819434	53.643725
3097.028372	250210.514140	53.648730
3096.321540	250061.163705	53.653735
3095.370535	249902.913355	53.658740
3094.927358	249753.699747	53.663745
3094.375184	249603.765005	53.668749
3093.828337	249453.931426	53.673754
3093.143941	249296.378012	53.678759
3092.532943	249143.855457	53.683764
3091.841735	248994.121564	53.688769
3091.033471	248845.832448	53.693773
3090.854804	248686.034992	53.698778
3089.932111	248535.217668	53.703783
3089.300639	248371.646812	53.708788
3088.735631	248211.045148	53.713793
3087.564124	248063.425468	53.718797
3087.268245	247906.575983	53.723802
3086.352831	247762.990639	53.728807
3085.524446	247605.665493	53.733812
3085.117948	247458.740260	53.738817
3084.134833	247314.096499	53.743821
3083.632165	247163.366892	53.748826
3082.996067	247013.142411	53.753831
3082.250956	246861.611114	53.758836
3082.182007	246708.368622	53.763841
3081.197241	246561.866874	53.768845
3080.580360	246413.957370	53.773850
3079.938910	246251.765625	53.778855
3079.095770	246092.992927	53.783860
3078.617630	245945.342084	53.788865
3077.497274	245790.102405	53.793869
3077.027361	245637.535716	53.798874
3076.094496	245489.728135	53.803879
3075.808384	245340.748805	53.808884
3074.927731	245190.488591	53.813889
3074.388806	245044.503601	53.818893
3073.936394	244893.080926	53.823898
3073.196362	244753.418058	53.828903
3072.349107	244604.095438	53.833908
3072.056461	244452.469721	53.838913
3070.709108	244298.897473	53.843917
3070.564791	244143.658018	53.848922
3069.748143	243999.500707	53.853927
3068.920362	243860.285586	53.858932
3068.611751	243707.109877	53.863937
3067.670989	243551.895317	53.868941
3067.067325	243397.264225	53.873946
3066.186008	243258.160091	53.878951
3065.608680	243108.236240	53.883956
3065.158338	242959.387469	53.888961
3063.979733	242812.818666	53.893965
3063.479777	242665.658792	53.898970
3062.895118	242523.096201	53.903975
3062.098990	242391.899169	53.908980
3061.898641	242233.640578	53.913985
3061.003780	242096.271499	53.918989
3060.570848	241949.967676	53.923994
3059.771755	241795.649614	53.928999
3059.276877	241650.247226	53.934004
3058.637090	241495.140388	53.939009
3057.578799	241342.875647	53.944013
3057.187884	241195.114595	53.949018
3056.391754	241045.762651	53.954023
3055.663243	240898.233651	53.959028
3055.379877	240752.722484	53.964033
3054.511537	240618.584910	53.969037
3054.059020	240469.332100	53.974042
3053.330176	240314.164508	53.979047
3052.348804	240155.344734	53.984052
3052.016778	240000.038363	53.989057
3051.058872	239864.719004	53.994061
3050.380945	239707.175973	53.999066
3050.253368	239568.084133	54.004071
3048.981369	239413.131044	54.009076
3048.460515	239264.450828	54.014081
3047.731929	239119.623330	54.019085
3047.429565	238972.156668	54.024090
3046.754953	238819.045130	54.029095
3046.117409	238665.673294	54.034100
3045.831755	238519.274081	54.039105
3044.368566	238365.167557	54.044109
3043.911020	238215.434690	54.049114
3043.334101	238065.695456	54.054119
3042.592953	237919.852951	54.059124
3042.029223	237762.702016	54.064129
3041.242471	237618.140333	54.069133
3040.984191	237467.969531	54.074138
3039.865971	237325.726992	54.079143
3039.200315	237171.674180	54.084148
3038.773148	237016.769002	54.089153
3037.580084	236881.821551	54.094157
3037.042897	236725.941123	54.099162
3036.406834	236576.060545	54.104167
3035.663924	236435.465866	54.109172
3034.918819	236290.670224	54.114177
3034.381189	236146.784097	54.119181
3033.814848	235996.791459	54.124186
3032.996439	235853.179353	54.129191
3032.397854	235721.907910	54.134196
3031.868012	235568.752644	54.139201
3031.060242	235427.252915	54.144205
3030.675084	235276.570601	54.149210
3029.605046	235137.455419	54.154215
3029.059318	234998.970412	54.159220
3028.791833	234843.330234	54.164225
3027.803839	234703.642471	54.169229
3027.320437	234556.770803	54.174234
3026.694239	234412.748364	54.179239
3025.956886	234263.829343	54.184244
3025.669899	234113.260550	54.189249
3024.804471	233970.015049	54.194253
3024.047576	233821.838216	54.199258
3023.407650	233677.920872	54.204263
3022.530880	233527.395403	54.209268
3022.042083	233385.593455	54.214273
3020.673737	233233.898566	54.219277
3020.890089	233080.527166	54.224282
3019.955236	232936.402975	54.229287
3018.684466	232792.001156	54.234292
3018.510639	232642.689862	54.239297
3017.970261	232508.739882	54.244301
3016.821477	232366.661964	54.249306
3016.704334	232228.800530	54.254311
3015.978883	232081.410739	54.259316
3015.264448	231931.778734	54.264321
3014.450565	231796.574468	54.269325
3013.913884	231636.958971	54.274330
3013.060232	231508.025175	54.279335
3012.417494	231357.160547	54.284340
3011.927928	231209.683869	54.289345
3011.165667	231073.530379	54.294349
3010.736383	230920.748468	54.299354
3009.916638	230793.847282	54.304359
3009.234778	230644.517746	54.309364
3008.853593	230501.124458	54.314369
3007.971767	230365.958507	54.319373
3007.557579	230204.136369	54.324378
3006.583713	230064.656893	54.329383
3005.839688	229924.784783	54.334388
3005.420442	229782.569911	54.339393
3004.657217	229634.757177	54.344397
3003.890966	229488.396491	54.349402
3003.063260	229346.628897	54.354407
3002.483378	229198.558711	54.359412
3002.030391	229052.862087	54.364417
3000.927820	228927.637860	54.369421
3000.505206	228772.974385	54.374426
2999.870356	228637.262734	54.379431
2998.887000	228503.465152	54.384436
2998.444198	228356.800536	54.389441
2997.971084	228229.695368	54.394445
2997.452436	228086.200437	54.399450
2996.406538	227941.719828	54.404455
2996.118347	227793.733162	54.409460
2995.461676	227654.080001	54.414465
2994.430901	227519.985918	54.419469
2994.114860	227376.536487	54.424474
2993.132941	227237.495640	54.429479
2992.500726	227107.896667	54.434484
2992.240444	226945.266910	54.439489
2991.344722	226803.717948	54.444493
2990.531859	226655.918164	54.449498
2989.896442	226525.544035	54.454503
2989.496296	226384.617510	54.459508
2988.965528	226240.083726	54.464513
2987.991442	226099.910519	54.469517
2987.243515	225946.042042	54.474522
2986.556081	225819.801902	54.479527
2985.857707	225683.150262	54.484532
2985.314702	225546.512447	54.489537
2984.715829	225400.361435	54.494541
2984.086181	225251.249401	54.499546
2983.250445	225114.327660	54.504551
2982.941730	224967.991460	54.509556
2982.289740	224824.497782	54.514561
2981.834278	224694.607284	54.519565
2981.216206	224537.398330	54.524570
2980.607944	224391.696182	54.529575
2979.420483	224242.216030	54.534580
2978.922624	224096.229612	54.539585
2978.127396	223957.623059	54.544589
2977.741017	223810.970284	54.549594
2976.742520	223668.373718	54.554599
2975.919137	223527.251831	54.559604
2975.407435	223381.548984	54.564609
2974.674474	223255.345543	54.569613
2974.175274	223105.147553	54.574618
2973.553697	222965.866032	54.579623
2972.683205	222823.339852	54.584628
2972.194453	222670.505960	54.589633
2971.342031	222533.884111	54.594637
2970.805546	222395.633992	54.599642
2970.125280	222262.447883	54.604647
2969.302859	222112.404825	54.609652
2969.073492	221960.778797	54.614657
2968.076970	221834.759428	54.619661
2967.193795	221687.030905	54.624666
2966.810374	221545.371991	54.629671
2965.898249	221412.020398	54.634676
2965.184939	221266.175254	54.639681
2964.528019	221137.837409	54.644685
2963.586399	220997.731795	54.649690
2963.064245	220867.323615	54.654695
2962.531962	220740.341513	54.659700
2962.366534	220601.704957	54.664705
2961.422714	220463.077319	54.669709
2960.948282	220312.473575	54.674714
2960.048993	220179.198526	54.679719
2959.335848	220038.180218	54.684724
2958.788294	219896.703165	54.689729
2957.896120	219760.830949	54.694733
2957.466575	219626.973361	54.699738
2956.960125	219492.899064	54.704743
2956.316680	219347.352139	54.709748
2955.578290	219201.311364	54.714753
2954.699620	219066.354813	54.719757
2954.202914	218928.206654	54.724762
2953.564731	218784.123887	54.729767
2952.789958	218647.420500	54.734772
2952.478797	218506.188772	54.739777
2951.397360	218372.844036	54.744781
2950.857413	218228.059461	54.749786
2949.757978	218091.879509	54.754791
2948.957166	217955.754375	54.759796
2948.738903	217820.644702	54.764801
2947.947760	217692.474189	54.769805
2947.430045	217545.408993	54.774810
2946.772179	217416.772367	54.779815
2946.106890	217283.071034	54.784820
2945.572728	217143.366608	54.789825
2944.398783	217002.796352	54.794829
2943.911454	216864.943485	54.799834
2943.459643	216739.801376	54.804839
2942.684886	216603.802025	54.809844
2942.337839	216466.156858	54.814849
2941.541960	216335.812960	54.819853
2940.862678	216196.375258	54.824858
2940.435947	216059.609070	54.829863
2939.490305	215918.355709	54.834868
2939.140139	215774.157144	54.839873
2937.562293	215654.503126	54.844877
2937.111557	215507.062516	54.849882
2936.815371	215370.200668	54.854887
2936.166167	215251.749568	54.859892
2935.320078	215102.157658	54.864897
2934.617449	214971.165174	54.869901
2934.219413	214844.299664	54.874906
2933.390138	214710.043788	54.879911
2932.919958	214570.754512	54.884916
2932.123289	214432.917338	54.889921
2931.338189	214309.563518	54.894925
2930.721957	214160.026414	54.899930
2930.074587	214031.318122	54.904935
2929.256220	213903.795427	54.909940
2929.010886	213765.846891	54.914945
2928.372676	213632.059340	54.919949
2927.941581	213501.981368	54.924954
2927.002261	213364.474477	54.929959
2926.303379	213222.233110	54.934964
2925.764065	213074.162752	54.939969
2924.948342	212938.915524	54.944973
2924.228620	212799.402193	54.949978
2923.622324	212666.871640	54.954983
2922.814354	212533.075026	54.959988
2922.176171	212399.926392	54.964993
2921.294554	212269.807651	54.969997
2920.766851	212134.300123	54.975002
2919.915282	212010.121107	54.980007
2919.318933	211871.964860	54.985012
2918.772599	211733.953726	54.990017
2918.167505	211614.076662	54.995021
2917.609899	211475.584211	55.000026
2916.853642	211340.674570	55.005031
2916.102534	211213.655623	55.010036
2915.436321	211073.462992	55.015041
2914.990740	210946.587122	55.020045
2914.216832	210807.073974	55.025050
2913.386360	210671.706582	55.030055
2912.895937	210541.885806	55.035060
2912.251805	210409.047733	55.040065
2911.312492	210283.638681	55.045069
2910.735073	210145.101372	55.050074
2910.447914	210007.854804	55.055079
2909.183488	209883.172591	55.060084
2908.402377	209744.592057	55.065089
2908.051342	209627.593142	55.070093
2907.607919	209492.472483	55.075098
2906.855486	209364.413845	55.080103
2906.013216	209231.940569	55.085108
2905.694388	209095.642860	55.090113
2904.699212	208966.490749	55.095117
2904.505626	208838.064721	55.100122
2903.666388	208702.906647	55.105127
2902.610540	208574.108606	55.110132
2902.521290	208439.430548	55.115137
2901.611120	208305.111855	55.120141
2901.013828	208172.920264	55.125146
2900.243603	208051.179862	55.130151
2899.360354	207913.739627	55.135156
2899.330022	207779.511880	55.140161
2897.941433	207658.684710	55.145165
2897.563239	207519.523617	55.150170
2896.900360	207384.480559	55.155175
2896.311921	207253.969544	55.160180
2895.607551	207126.595268	55.165185
2894.776716	207002.639374	55.170189
2894.499688	206867.676385	55.175194
2893.722841	206730.311105	55.180199
2892.731577	206602.907015	55.185204
2892.227069	206460.688499	55.190209
2891.743205	206334.871856	55.195213
2890.944615	206210.403441	55.200218
2890.663829	206069.232218	55.205223
2889.665384	205938.318129	55.210228
2888.782457	205805.527950	55.215233
2887.944243	205674.003655	55.220237
2887.548602	205540.004253	55.225242
2887.064020	205420.323903	55.230247
2885.717926	205295.536874	55.235252
2885.471364	205159.618488	55.240257
2884.580985	205041.301276	55.245261
2883.717433	204909.948165	55.250266
2883.351523	204790.517578	55.255271
2882.551739	204671.079580	55.260276
2881.801991	204544.838021	55.265281
2881.245578	204424.254805	55.270285
2880.871103	204301.505011	55.275290
2880.288293	204164.471388	55.280295
2879.377304	204038.549179	55.285300
2878.980961	203914.441968	55.290305
2878.022933	203797.079772	55.295309
2877.867003	203665.630191	55.300314
2876.880904	203548.158418	55.305319
2876.193535	203409.628754	55.310324
2875.719587	203275.163437	55.315329
2874.847246	203151.578677	55.320333
2874.074894	203019.515541	55.325338
2873.472091	202893.381639	55.330343
2872.932414	202773.219235	55.335348
2872.413767	202636.879074	55.340353
2871.868905	202518.308780	55.345357
2871.139331	202383.555198	55.350362
2870.769546	202256.889522	55.355367
2869.648290	202119.742507	55.360372
2869.229311	201986.709594	55.365377
2868.252991	201865.816557	55.370381
2867.737308	201728.154670	55.375386
2867.335502	201607.998398	55.380391
2866.115149	201480.552927	55.385396
2866.124547	201346.384763	55.390401
2865.230069	201218.188387	55.395405
2864.295061	201090.571380	55.400410
2863.794673	200960.493443	55.405415
2863.302451	200828.709300	55.410420
2862.482841	200694.355863	55.415425
2861.803633	200561.151268	55.420429
2861.344523	200434.402121	55.425434
2860.750173	200306.223987	55.430439
2859.890139	200183.598318	55.435444
2859.148523	200042.744196	55.440449
2858.252510	199911.306175	55.445453
2857.743625	199781.601437	55.450458
2856.962438	199657.450168	55.455463
2856.216318	199535.991381	55.460468
2855.677611	199404.447117	55.465473
2854.733902	199286.990444	55.470477
2854.251352	199160.680657	55.475482
2853.724554	199026.157753	55.480487
2852.961771	198903.010601	55.485492
2852.685178	198766.310919	55.490497
2852.072004	198646.652783	55.495501
2851.581268	198522.101857	55.500506
2850.916624	198390.758185	55.505511
2849.736039	198254.101172	55.510516
2849.369393	198122.163807	55.515521
2848.401391	197993.299616	55.520525
2847.925810	197864.624985	55.525530
2847.237690	197739.407297	55.530535
2846.323827	197610.064656	55.535540
2845.817374	197480.517847	55.540545
2844.926814	197354.137012	55.545549
2844.290564	197224.980407	55.550554
2843.873410	197108.768565	55.555559
2843.254537	196978.375528	55.560564
2842.417987	196848.577171	55.565569
2841.910140	196736.846851	55.570573
2841.009624	196597.375867	55.575578
2840.307722	196474.288399	55.580583
2839.716766	196341.131331	55.585588
2839.626312	196210.287541	55.590593
2838.459591	196095.430943	55.595597
2837.774033	195961.399132	55.600602
2837.270686	195832.848451	55.605607
2836.320810	195723.697022	55.610612
2835.983438	195584.470439	55.615617
2834.984803	195460.796178	55.620621
2834.587097	195338.999306	55.625626
2833.996165	195207.104880	55.630631
2833.175586	195085.184720	55.635636
2832.628535	194962.687124	55.640641
2831.592331	194837.035370	55.645645
2830.919060	194703.259406	55.650650
2830.429572	194591.378177	55.655655
2830.027716	194462.725822	55.660660
2829.634050	194334.835935	55.665665
2828.498919	194209.252309	55.670669
2827.815629	194088.801516	55.675674
2827.203725	193957.384461	55.680679
2826.364915	193829.299157	55.685684
2826.049263	193694.833053	55.690689
2825.259103	193580.202461	55.695693
2824.548538	193456.589295	55.700698
2823.887640	193332.968570	55.705703
2823.106785	193211.784648	55.710708
2822.740450	193073.243952	55.715713
2822.036853	192950.381638	55.720717
2821.310621	192826.708906	55.725722
2820.610788	192698.782641	55.730727
2819.900080	192577.309248	55.735732
2819.200557	192448.925537	55.740737
2818.460310	192328.958807	55.745741
2817.957220	192200.150211	55.750746
2817.253235	192074.783635	55.755751
2816.155347	191955.014417	55.760756
2816.170792	191821.760591	55.765761
2815.194637	191700.636771	55.770765
2814.613532	191585.977718	55.775770
2814.102096	191454.793164	55.780775
2813.241421	191330.509345	55.785780
2812.907331	191199.590028	55.790785
2812.181849	191079.255066	55.795789
2811.673264	190946.900909	55.800794
2811.240982	190819.942327	55.805799
2810.010351	190695.744178	55.810804
2809.675637	190555.755196	55.815809
2808.663022	190436.663274	55.820813
2807.939366	190307.958253	55.825818
2807.541015	190184.151260	55.830823
2806.889088	190054.608574	55.835828
2806.265733	189925.036269	55.840833
2805.312724	189810.338563	55.845837
2804.927616	189668.362682	55.850842
2804.340311	189542.488028	55.855847
2803.191764	189418.152978	55.860852
2802.816913	189286.978167	55.865857
2802.105478	189172.409140	55.870861
2801.320016	189052.152398	55.875866
2800.702598	188917.391095	55.880871
2800.176591	188794.587579	55.885876
2799.458311	188665.339096	55.890881
2798.552125	188540.586304	55.895885
2798.023102	188424.247234	55.900890
2797.188558	188291.888481	55.905895
2796.588772	188181.222679	55.910900
2796.542253	188047.213134	55.915905
2795.536524	187926.001826	55.920909
2794.857810	187802.041929	55.925914
2794.239111	187673.034864	55.930919
2793.594448	187548.268751	55.935924
2792.722479	187423.767974	55.940929
2792.117865	187294.123625	55.945933
2791.347475	187168.055352	55.950938
2791.170691	187040.862924	55.955943
2789.596974	186915.889444	55.960948
2789.417995	186790.148364	55.965953
2788.969212	186675.785596	55.970957
2788.214163	186553.456824	55.975962
2787.612141	186426.816875	55.980967
2786.808866	186301.099678	55.985972
2786.366927	186169.486298	55.990977
2785.316826	186051.696390	55.995981
2784.809214	185923.694377	56.000986
2784.039844	185801.166341	56.005991
2783.060312	185684.294892	56.010996
2782.801254	185558.302728	56.016001
2782.050447	185442.769610	56.021005
2781.181423	185314.559402	56.026010
2780.642732	185196.067363	56.031015
2779.786828	185074.318290	56.036020
2779.557925	184956.553825	56.041025
2778.822723	184840.599970	56.046029
2778.545764	184711.661633	56.051034
2777.732109	184585.467431	56.056039
2776.767850	184464.335075	56.061044
2776.136312	184332.362710	56.066049
2775.552413	184209.071793	56.071053
2774.880073	184092.550183	56.076058
2774.220174	183966.587799	56.081063
2773.405540	183846.934519	56.086068
2772.979078	183715.771092	56.091073
2772.089441	183604.475384	56.096077
2771.414006	183471.990957	56.101082
2770.995683	183343.549641	56.106087
2770.203321	183222.775071	56.111092
2769.842448	183099.426467	56.116097
2768.967562	182975.218276	56.121101
2768.506025	182852.725885	56.126106
2767.769371	182730.926171	56.131111
2767.183424	182607.042159	56.136116
2766.554868	182464.363993	56.141121
2765.580269	182355.272865	56.146125
2765.091341	182230.433218	56.151130
2764.441525	182100.556600	56.156135
2763.844972	181978.978480	56.161140
2763.271581	181853.021157	56.166145
2762.458060	181727.407526	56.171149
2761.970644	181594.657297	56.176154
2761.168978	181467.388878	56.181159
2760.347116	181351.928571	56.186164
2759.435808	181218.457969	56.191169
2758.961883	181103.515633	56.196173
2758.450582	180978.148874	56.201178
2757.550498	180849.002539	56.206183
2757.016096	180734.833980	56.211188
2756.363693	180603.931920	56.216193
2755.973189	180482.935936	56.221197
2755.314928	180352.773338	56.226202
2754.579262	180230.853287	56.231207
2753.941785	180108.065789	56.236212
2753.779856	179970.384514	56.241217
2752.707196	179854.611796	56.246221
2752.218209	179718.038896	56.251226
2751.566670	179578.350370	56.256231
2750.498598	179468.187448	56.261236
2749.770026	179334.312180	56.266241
2749.140896	179211.449628	56.271245
2748.579484	179083.119939	56.276250
2748.063201	178954.719892	56.281255
2747.283965	178833.713850	56.286260
2747.005077	178696.551299	56.291265
2746.166852	178570.938134	56.296269
2745.350916	178435.375131	56.301274
2744.747451	178302.488164	56.306279
2743.720994	178178.864791	56.311284
2743.394551	178051.734817	56.316289
2742.644757	177929.403899	56.321293
2741.822743	177808.725575	56.326298
2741.505949	177673.251329	56.331303
2740.559872	177546.310078	56.336308
2740.061909	177411.514063	56.341313
2739.156214	177296.090804	56.346317
2738.836610	177170.526895	56.351322
2738.089678	177033.876389	56.356327
2737.037029	176916.188026	56.361332
2736.472443	176788.997880	56.366337
2735.766030	176666.167771	56.371341
2735.581707	176527.382064	56.376346
2734.999643	176413.525315	56.381351
2733.732588	176290.530754	56.386356
2733.580864	176156.243621	56.391361
2732.637081	176030.934678	56.396365
2732.100980	175905.103665	56.401370
2731.383086	175774.646781	56.406375
2730.527258	175656.447541	56.411380
2730.036465	175520.880738	56.416385
2729.476009	175406.908899	56.421389
2728.959845	175287.232441	56.426394
2728.025877	175147.107523	56.431399
2727.408230	175020.808853	56.436404
2727.115003	174894.179381	56.441409
2726.102604	174765.145979	56.446413
2725.346648	174642.291650	56.451418
2724.911820	174515.316961	56.456423
2724.055731	174385.051772	56.461428
2723.131882	174258.473313	56.466433
2722.509788	174135.192342	56.471437
2722.089457	174009.450618	56.476442
2721.899799	173883.176740	56.481447
2720.770948	173763.372925	56.486452
2720.407457	173623.569915	56.491457
2719.756246	173508.091650	56.496461
2718.748823	173373.491441	56.501466
2718.565709	173246.709815	56.506471
2717.772365	173107.905111	56.511476
2717.204680	172969.891804	56.516481
2716.554251	172851.375754	56.521485
2715.557378	172724.012503	56.526490
2715.242236	172587.410346	56.531495
2714.351753	172461.124812	56.536500
2713.877180	172319.258281	56.541505
2713.008648	172204.835643	56.546509
2712.460803	172070.001729	56.551514
2712.236956	171933.539981	56.556519
2711.180737	171807.816929	56.561524
2710.623091	171667.174066	56.566529
2709.944207	171541.710028	56.571533
2709.170911	171393.916986	56.576538
2708.755493	171267.699920	56.581543
2707.625668	171137.654084	56.586548
2707.343072	171006.279052	56.591553
2706.508591	170881.681118	56.596557
2705.981210	170743.453045	56.601562
2704.957365	170608.852175	56.606567
2704.085683	170483.638273	56.611572
2703.851877	170354.152553	56.616577
2702.777816	170229.264024	56.621581
2702.241706	170099.903345	56.626586
2702.127952	169973.947897	56.631591
2701.173686	169846.104033	56.636596
2700.618765	169709.549917	56.641601
2699.886651	169572.744588	56.646605
2699.214108	169439.020465	56.651610
2698.487798	169311.600067	56.656615
2697.884842	169187.085371	56.661620
2697.213051	169050.361364	56.666625
2696.394107	168929.264329	56.671629
2695.786030	168801.877764	56.676634
2695.576363	168662.157146	56.681639
2694.609273	168540.042068	56.686644
2694.044002	168407.944972	56.691649
2693.335913	168275.514902	56.696653
2692.536830	168139.399278	56.701658
2691.867410	168006.646114	56.706663
2691.461583	167877.272308	56.711668
2690.429634	167731.963097	56.716673
2690.180624	167606.774411	56.721677
2689.339570	167469.141917	56.726682
2688.789338	167343.111702	56.731687
2687.802271	167216.896792	56.736692
2687.656878	167079.409836	56.741697
2686.607117	166954.248445	56.746701
2686.138730	166820.730089	56.751706
2685.339692	166694.016666	56.756711
2684.651518	166560.305174	56.761716
2683.708664	166417.886118	56.766721
2683.062283	166287.881958	56.771725
2682.429636	166163.381928	56.776730
2682.205859	166020.659738	56.781735
2681.122540	165908.210002	56.786740
2680.499809	165774.338376	56.791745
2679.947530	165650.221511	56.796749
2679.637184	165524.057705	56.801754
2679.000104	165386.260703	56.806759
2678.208331	165251.743832	56.811764
2677.651608	165110.578293	56.816769
2676.873631	164986.486697	56.821773
2676.422657	164854.206020	56.826778
2675.655760	164706.450736	56.831783
2674.766412	164581.399087	56.836788
2674.526158	164434.235362	56.841793
2673.608600	164307.472592	56.846797
2672.593047	164167.616716	56.851802
2672.297033	164035.428874	56.856807
2671.586102	163904.375289	56.861812
2671.094725	163763.827604	56.866817
2670.277967	163645.328477	56.871821
2669.999340	163508.727780	56.876826
2669.391049	163358.079302	56.881831
2668.396942	163220.855590	56.886836
2667.736464	163084.787422	56.891841
2667.023191	162949.808860	56.896845
2666.615657	162812.519195	56.901850
2665.762766	162668.027982	56.906855
2664.952519	162534.083487	56.911860
2664.801235	162394.313663	56.916865
2663.621104	162267.841189	56.921869
2663.141488	162128.315128	56.926874
2662.553720	161999.232342	56.931879
2661.589046	161861.335293	56.936884
2661.069461	161712.243469	56.941889
2660.240617	161585.234616	56.946893
2659.487466	161446.873377	56.951898
2659.192572	161319.310460	56.956903
2658.205926	161184.686977	56.961908
2658.099346	161043.580384	56.966913
2656.965657	160912.591949	56.971917
2656.075764	160769.792476	56.976922
2655.713357	160628.689920	56.981927
2655.037705	160505.703594	56.986932
2654.563385	160378.248761	56.991937
2653.931599	160238.906768	56.996941
2653.038878	160106.688068	57.001946
2652.445307	159966.438439	57.006951
2651.315564	159832.681856	57.011956
2650.990945	159686.949406	57.016961
2650.348722	159561.570972	57.021965
2649.376617	159431.325232	57.026970
2649.243821	159284.877544	57.031975
2648.787380	159169.819601	57.036980
2647.887710	159015.002170	57.041985
2647.381937	158884.532024	57.046989
2646.573994	158748.541956	57.051994
2646.201939	158614.593703	57.056999
2645.398100	158484.922340	57.062004
2644.859685	158331.919501	57.067009
2644.093590	158197.043686	57.072013
2642.857280	158050.178519	57.077018
2642.548261	157916.540787	57.082023
2641.827887	157789.426760	57.087028
2641.580201	157646.767101	57.092033
2640.627043	157509.838740	57.097037
2640.014242	157360.004687	57.102042
2639.448180	157225.139108	57.107047
2638.525017	157101.644649	57.112052
2638.406226	156950.284898	57.117057
2637.704816	156827.035962	57.122061
2636.819799	156679.574352	57.127066
2636.207341	156535.515188	57.132071
2635.568189	156395.592297	57.137076
2634.915895	156244.282056	57.142081
2634.333183	156109.639609	57.147085
2633.914338	155970.268308	57.152090
2633.028188	155816.429204	57.157095
2632.215609	155683.858766	57.162100
2631.720207	155534.026821	57.167105
2631.005888	155385.946307	57.172109
2629.745058	155247.639334	57.177114
2629.203863	155112.740028	57.182119
2628.479051	154974.946689	57.187124
2627.950378	154837.987220	57.192129
2627.000295	154707.209298	57.197133
2626.676695	154569.443027	57.202138
2626.268954	154428.944993	57.207143
2625.109821	154301.277926	57.212148
2624.957035	154160.766040	57.217153
2624.331172	154020.838147	57.222157
2623.749741	153883.712967	57.227162
2623.133785	153738.801906	57.232167
2622.423027	153619.214222	57.237172
2622.123853	153404.394455	57.242177
2621.164951	153261.382898	57.247181
2620.086481	153107.357860	57.252186
2619.765569	152958.666444	57.257191
2619.308822	152828.605774	57.262196
2618.788819	152677.951569	57.267201
2617.943883	152535.713144	57.272205
2617.205752	152385.031281	57.277210
2616.772631	152246.109870	57.282215
2615.794435	152098.594146	57.287220
2615.295820	151941.851585	57.292225
2614.412198	151811.316007	57.297229
2614.009040	151660.190358	57.302234
2613.483530	151507.902737	57.307239
2612.324995	151380.145139	57.312244
2611.699550	151227.798392	57.317249
2611.490786	151076.365007	57.322253
2610.716575	150940.350222	57.327258
2609.988980	150788.174229	57.332263
2608.835149	150640.819995	57.337268
2608.525091	150493.891963	57.342273
2607.790662	150367.113340	57.347277
2607.162760	150214.771712	57.352282
2606.689908	150058.491644	57.357287
2605.871964	149922.437205	57.362292
2605.637365	149765.726797	57.367297
2604.823079	149634.782239	57.372301
2603.938330	149483.539639	57.377306
2603.466172	149344.382568	57.382311
2602.655256	149198.340467	57.387316
2601.970394	149035.324852	57.392321
2601.107606	148896.536637	57.397325
2600.689907	148751.247649	57.402330
2599.974661	148606.120848	57.407335
2599.204401	148465.489723	57.412340
2598.373603	148321.450084	57.417345
2597.586188	148169.270490	57.422349
2597.194169	148037.045475	57.427354
2596.610430	147891.113130	57.432359
2596.006025	147753.966495	57.437364
2595.603623	147599.301235	57.442369
2594.965120	147450.609084	57.447373
2594.064263	147310.118126	57.452378
2593.639949	147146.105011	57.457383
2592.667126	147011.396459	57.462388
2592.117321	146863.531766	57.467393
2591.450103	146717.694292	57.472397
2590.848853	146568.924126	57.477402
2590.330686	146425.085007	57.482407
2589.477652	146282.913547	57.487412
2588.985194	146128.295162	57.492417
2588.372125	145993.699157	57.497421
2587.374438	145839.149546	57.502426
2586.857445	145681.665236	57.507431
2586.119565	145534.039918	57.512436
2585.530465	145385.680082	57.517441
2585.023145	145244.221019	57.522445
2583.973536	145095.160362	57.527450
2583.693808	144933.690123	57.532455
2582.897588	144800.640486	57.537460
2582.558586	144656.387163	57.542465
2581.675357	144496.844708	57.547469
2580.949694	144358.296157	57.552474
2580.099186	144203.642380	57.557479
2579.423426	144060.842998	57.562484
2578.696502	143899.194856	57.567489
2578.286527	143759.861940	57.572493
2577.177457	143608.365370	57.577498
2576.729666	143463.130984	57.582503
2575.950011	143331.965678	57.587508
2575.578971	143176.211803	57.592513
2575.080957	143030.110641	57.597517
2573.827570	142889.555683	57.602522
2573.398673	142736.367276	57.607527
2572.525146	142595.397683	57.612532
2572.229058	142451.884856	57.617537
2571.586861	142317.754171	57.622541
2570.761327	142176.054633	57.627546
2570.513061	142016.411715	57.632551
2569.733006	141872.775001	57.637556
2568.988609	141727.684793	57.642561
2568.705262	141570.514799	57.647565
2567.902301	141435.320740	57.652570
2567.377657	141275.179143	57.657575
2566.369636	141124.047361	57.662580
2565.926386	140971.378350	57.667585
2565.488280	140826.561569	57.672589
2564.582917	140667.588940	57.677594
2563.911857	140519.062317	57.682599
2562.864956	140368.690123	57.687604
2562.628718	140216.513063	57.692609
2562.116332	140062.868565	57.697613
2561.168282	139908.544266	57.702618
2560.921375	139751.263620	57.707623
2559.956460	139604.986135	57.712628
2559.241730	139451.961285	57.717633
2558.109139	139300.083390	57.722637
2557.946335	139150.542809	57.727642
2557.447223	138993.090129	57.732647
2556.216321	138852.537699	57.737652
2555.873802	138696.230644	57.742657
2555.612326	138554.789100	57.747661
2554.770935	138396.618818	57.752666
2554.083076	138237.345136	57.757671
2553.435110	138084.583542	57.762676
2552.799562	137936.788314	57.767681
2552.192184	137775.725703	57.772685
2551.567385	137616.661351	57.777690
2551.156926	137462.582172	57.782695
2549.910149	137319.905184	57.787700
2549.485125	137156.619188	57.792705
2549.022217	137005.688696	57.797709
2548.102656	136852.785966	57.802714
2547.486923	136701.919369	57.807719
2546.655510	136542.487043	57.812724
2546.192160	136387.240407	57.817729
2545.551925	136235.973568	57.822733
2544.458109	136084.360166	57.827738
2544.563493	135916.423618	57.832743
2543.596571	135780.277680	57.837748
2542.861951	135609.998785	57.842753
2542.180365	135447.588738	57.847757
2541.405109	135300.730914	57.852762
2540.900995	135147.847511	57.857767
2540.216635	134997.165768	57.862772
2539.788479	134827.427259	57.867777
2538.914165	134684.284944	57.872781
2538.240505	134524.292451	57.877786
2537.602550	134369.643220	57.882791
2536.727090	134214.498930	57.887796
2536.218453	134064.746943	57.892801
2535.626114	133909.191043	57.897805
2534.616708	133742.434620	57.902810
2534.198318	133596.722993	57.907815
2533.321900	133445.571701	57.912820
2533.029529	133302.864854	57.917825
2532.199618	133140.694569	57.922829
2531.413885	132992.922900	57.927834
2531.186368	132823.278765	57.932839
2530.759969	132665.950387	57.937844
2529.595989	132508.879502	57.942849
2529.104784	132359.667185	57.947853
2528.366333	132185.331775	57.952858
2528.034727	132042.040462	57.957863
2527.268343	131884.389235	57.962868
2526.207936	131729.960983	57.967873
2525.724613	131575.086462	57.972877
2524.806386	131417.944577	57.977882
2524.159408	131261.446474	57.982887
2523.708981	131113.669569	57.987892
2522.999447	130954.376009	57.992897
2522.347581	130790.285720	57.997901
2521.347052	130635.904787	58.002906
2520.860539	130479.017265	58.007911
2520.211178	130347.432142	58.012916
2519.744430	130175.619084	58.017921
2519.217666	130015.298492	58.022925
2518.180035	129875.889672	58.027930
2517.993604	129721.613381	58.032935
2517.003209	129561.318074	58.037940
2516.337813	129394.012069	58.042945
2515.778212	129254.073367	58.047949
2515.067419	129100.518669	58.052954
2514.551797	128937.738561	58.057959
2513.255731	128779.629937	58.062964
2512.915867	128632.039156	58.067969
2512.475496	128485.989154	58.072973
2511.458441	128333.007975	58.077978
2511.015010	128167.833272	58.082983
2510.416235	128017.861038	58.087988
2509.994128	127861.041594	58.092993
2509.188782	127708.195434	58.097997
2508.642169	127543.002733	58.103002
2507.995262	127388.418730	58.108007
2507.139570	127228.687115	58.113012
2506.450145	127065.983710	58.118017
2506.173559	126918.874682	58.123021
2505.024919	126764.576922	58.128026
2504.507162	126603.855616	58.133031
2503.983456	126447.149265	58.138036
2503.226631	126292.779374	58.143041
2502.575226	126138.177760	58.148045
2501.825501	125985.573708	58.153050
2501.162632	125822.086159	58.158055
2500.635610	125677.309400	58.163060
2500.053084	125519.690677	58.168065
2499.356946	125339.080177	58.173069
2498.731117	125192.670793	58.178074
2498.019448	125026.224221	58.183079
2497.220258	124885.444201	58.188084
2496.810332	124715.256359	58.193089
2496.195388	124555.502311	58.198093
2495.285869	124394.284766	58.203098
2494.879945	124229.928023	58.208103
2494.148685	124083.820747	58.213108
2493.793796	123917.819723	58.218113
2492.958800	123751.286306	58.223117
2492.333406	123597.393540	58.228122
2491.583397	123422.810717	58.233127
2490.765049	123269.851991	58.238132
2490.096741	123100.324862	58.243137
2489.404567	122947.576551	58.248141
2488.965298	122782.497511	58.253146
2488.474657	122614.583338	58.258151
2487.504563	122463.316708	58.263156
2486.987336	122296.297602	58.268161
2486.633874	122148.185621	58.273165
2485.401631	121978.894711	58.278170
2484.857496	121818.891881	58.283175
2484.221300	121660.174344	58.288180
2483.252285	121499.821783	58.293185
2482.416719	121338.649125	58.298189
2482.030667	121179.907527	58.303194
2481.644004	121027.096485	58.308199
2480.566099	120857.293136	58.313204
2480.284536	120702.207272	58.318209
2479.637151	120541.098556	58.323213
2478.722233	120392.641056	58.328218
2478.326966	120230.999114	58.333223
2477.640890	120061.621289	58.338228
2476.904249	119888.196060	58.343233
2476.024711	119738.067090	58.348237
2475.350875	119585.183021	58.353242
2475.080959	119416.225883	58.358247
2474.204134	119267.635439	58.363252
2473.646548	119090.581436	58.368257
2473.034001	118941.779570	58.373261
2472.158463	118780.006932	58.378266
2471.932242	118617.396024	58.383271
2470.831065	118462.358190	58.388276
2470.199057	118298.670989	58.393281
2469.601343	118141.181189	58.398285
2468.949752	117988.417277	58.403290
2468.798987	117810.285564	58.408295
2467.719469	117658.118304	58.413300
2466.892501	117487.846529	58.418305
2466.471488	117326.518774	58.423309
2465.588507	117162.345384	58.428314
2465.124809	117005.050770	58.433319
2464.274982	116838.804908	58.438324
2463.741736	116671.221416	58.443329
2463.205895	116522.580065	58.448333
2462.190527	116350.200301	58.453338
2461.971284	116198.939972	58.458343
2461.274600	116033.912806	58.463348
2460.362961	115873.833545	58.468353
2459.919218	115713.224126	58.473357
2459.187960	115549.957410	58.478362
2458.355539	115381.166749	58.483367
2457.692667	115220.588837	58.488372
2457.240819	115052.895205	58.493377
2456.889336	114888.817253	58.498381
2456.018970	114736.907213	58.503386
2455.537567	114555.861232	58.508391
2454.856146	114409.660818	58.513396
2454.250343	114228.294178	58.518401
2453.678427	114056.234201	58.523405
2452.644617	113898.173368	58.528410
2451.954135	113729.466464	58.533415
2450.983408	113568.376682	58.538420
2450.875147	113390.922923	58.543425
2449.872033	113234.530571	58.548429
2449.228553	113062.780700	58.553434
2448.871268	112907.538285	58.558439
2447.734618	112743.440154	58.563444
2447.398421	112573.758307	58.568449
2446.427867	112411.216291	58.573453
2445.820198	112244.004037	58.578458
2445.473598	112078.217514	58.583463
2444.679305	111918.081410	58.588468
2444.287181	111758.136435	58.593473
2443.246275	111586.573991	58.598477
2442.552207	111425.892104	58.603482
2441.959644	111253.956283	58.608487
2441.473561	111099.481734	58.613492
2440.325600	110950.132754	58.618497
2439.796208	110776.895661	58.623501
2439.094206	110611.391075	58.628506
2438.632774	110448.343389	58.633511
2437.791197	110300.536250	58.638516
2437.504880	110134.099604	58.643521
2436.598162	109977.484106	58.648525
2435.662457	109811.038375	58.653530
2435.420973	109647.320232	58.658535
2434.657028	109480.069009	58.663540
2433.886139	109320.847176	58.668545
2432.728553	109160.564526	58.673549
2432.465540	108999.474841	58.678554
2432.102903	108833.681005	58.683559
2431.351303	108689.016691	58.688564
2430.702480	108515.529000	58.693569
2430.236254	108352.927544	58.698573
2429.074327	108198.654596	58.703578
2428.786683	108026.769260	58.708583
2427.982977	107862.949200	58.713588
2427.376182	107708.324876	58.718593
2426.672769	107541.953033	58.723597
2426.149081	107375.807648	58.728602
2425.569666	107220.344562	58.733607
2424.972460	107054.961755	58.738612
2424.255418	106889.262801	58.743617
2423.869419	106714.534493	58.748621
2423.220446	106553.845865	58.753626
2422.341904	106390.967683	58.758631
2421.858998	106218.694751	58.763636
2421.058012	106045.204542	58.768641
2420.446521	105873.379575	58.773645
2419.513277	105710.286291	58.778650
2418.945049	105534.802401	58.783655
2418.532093	105382.198938	58.788660
2417.596447	105208.393555	58.793665
2417.234057	105042.936667	58.798669
2416.046088	104878.944137	58.803674
2415.698285	104696.395545	58.808679
2415.046945	104548.117663	58.813684
2414.461821	104384.521491	58.818689
2413.903306	104215.612116	58.823693
2413.247454	104042.938250	58.828698
2412.794906	103860.983676	58.833703
2411.590622	103706.156434	58.838708
2411.272755	103533.274109	58.843713
2410.901510	103358.771109	58.848717
2409.654166	103198.593358	58.853722
2408.987934	103012.936279	58.858727
2408.450776	102854.836926	58.863732
2407.880997	102694.295099	58.868737
2407.307060	102526.307446	58.873741
2406.371450	102356.342003	58.878746
2405.967654	102184.314255	58.883751
2404.773697	102011.448813	58.888756
2404.086313	101842.887753	58.893761
2403.472224	101688.272074	58.898765
2402.803529	101521.404100	58.903770
2402.394330	101360.084760	58.908775
2401.778481	101186.277421	58.913780
2401.046039	101023.520963	58.918785
2400.190070	100857.328124	58.923789
2399.484388	100698.413752	58.928794
2399.302366	100517.247884	58.933799
2398.591824	100370.705812	58.938804
2397.744746	100200.443956	58.943809
2396.901567	100029.909985	58.948813
2396.489264	99859.581712	58.953818
2396.059662	99694.845616	58.958823
2395.292993	99534.014307	58.963828
2394.572882	99366.389833	58.968833
2393.794727	99201.731555	58.973837
2393.257524	99035.069984	58.978842
2392.691472	98853.381845	58.983847
2391.927617	98698.321513	58.988852
2391.144779	98521.414731	58.993857
2390.929940	98353.134025	58.998861
2390.369733	98180.107984	59.003866
2389.905496	98014.774209	59.008871
2388.770935	97839.653637	59.013876
2388.325732	97661.114367	59.018881
2387.596989	97498.515463	59.023885
2386.764487	97323.794936	59.028890
2386.185109	97139.858330	59.033895
2385.452760	96984.620728	59.038900
2384.755112	96811.804460	59.043905
2384.018251	96634.048853	59.048909
2383.604927	96453.478192	59.053914
2382.809779	96285.317472	59.058919
2382.038308	96119.405660	59.063924
2381.630838	95953.722743	59.068929
2381.149249	95779.751239	59.073933
2380.047170	95606.786342	59.078938
2379.469494	95415.329372	59.083943
2379.028348	95247.576877	59.088948
2378.356885	95082.011990	59.093953
2377.420743	94911.347203	59.098957
2376.929505	94742.027356	59.103962
2376.454757	94567.721704	59.108967
2375.332753	94387.527304	59.113972
2374.954824	94217.115404	59.118977
2374.207194	94042.032727	59.123981
2373.377719	93889.748933	59.128986
2373.130200	93703.574660	59.133991
2371.908231	93541.811795	59.138996
2371.841724	93374.413452	59.144001
2371.053531	93194.594292	59.149005
2370.383368	93023.388142	59.154010
2369.810941	92843.429818	59.159015
2368.955677	92665.293286	59.164020
2368.451185	92498.624116	59.169025
2367.829878	92321.518540	59.174029
2366.612549	92146.563328	59.179034
2366.053028	91980.819875	59.184039
2365.753991	91815.258293	59.189044
2364.588868	91637.458177	59.194049
2364.271029	91464.781575	59.199053
2363.260236	91304.320461	59.204058
2362.869130	91130.206099	59.209063
2361.995186	90965.458554	59.214068
2361.289761	90792.163916	59.219073
2360.807511	90625.587825	59.224077
2359.878356	90453.307770	59.229082
2359.558590	90277.952492	59.234087
2359.063846	90116.574991	59.239092
2358.360375	89945.347346	59.244097
2357.563407	89777.724417	59.249101
2357.055295	89597.883913	59.254106
2356.377425	89430.992905	59.259111
2355.225812	89259.106264	59.264116
2354.907266	89100.669149	59.269121
2354.204563	88918.322784	59.274125
2353.545711	88761.374932	59.279130
2352.769954	88591.652947	59.284135
2351.862738	88416.843266	59.289140
2351.155057	88249.566670	59.294145
2350.928511	88089.188743	59.299149
2350.000862	87930.368615	59.304154
2349.875720	87745.037003	59.309159
2348.862162	87587.088872	59.314164
2347.965129	87422.511325	59.319169
2347.685000	87250.255238	59.324173
2347.042592	87079.072279	59.329178
2346.333399	86906.639744	59.334183
2345.665227	86738.899510	59.339188
2344.758842	86571.039880	59.344193
2344.418512	86405.684542	59.349197
2343.731773	86237.361635	59.354202
2342.991117	86057.663585	59.359207
2342.540728	85891.042842	59.364212
2341.567396	85722.217944	59.369217
2341.223116	85559.741345	59.374221
2340.142570	85387.849031	59.379226
2339.813275	85223.914673	59.384231
2339.118909	85055.323402	59.389236
2338.592510	84870.226098	59.394241
2338.022271	84703.462512	59.399245
2337.249409	84528.897806	59.404250
2336.728330	84346.998901	59.409255
2335.636052	84183.580222	59.414260
2334.845607	84012.572146	59.419265
2334.384491	83844.771190	59.424269
2333.898090	83669.065274	59.429274
2332.901299	83504.666939	59.434279
2332.501837	83335.282015	59.439284
2331.740716	83161.100718	59.444289
2331.299506	82991.268831	59.449293
2330.360798	82823.222162	59.454298
2330.185723	82639.280281	59.459303
2328.965317	82478.969123	59.464308
2328.671642	82311.090473	59.469313
2328.102415	82123.514243	59.474317
2327.182531	81966.334657	59.479322
2326.607405	81780.213816	59.484327
2326.142032	81618.921248	59.489332
2325.547599	81447.072750	59.494337
2324.970912	81261.457464	59.499341
2323.845470	81103.493085	59.504346
2323.366028	80917.320415	59.509351
2322.782242	80738.732927	59.514356
2322.112327	80570.110418	59.519361
2321.137616	80393.653898	59.524365
2320.524686	80231.761752	59.529370
2319.778342	80062.800600	59.534375
2319.045671	79884.370831	59.539380
2318.859597	79724.005615	59.544385
2317.977832	79544.784926	59.549389
2317.193800	79373.623730	59.554394
2317.081399	79203.434745	59.559399
2316.302696	79028.581086	59.564404
2315.532956	78847.650389	59.569409
2315.364879	78678.139952	59.574413
2314.271284	78495.799895	59.579418
2314.073997	78314.345878	59.584423
2313.086745	78139.513851	59.589428
2312.313461	77953.370165	59.594433
2311.783105	77774.483057	59.599437
2310.787294	77590.792200	59.604442
2310.532739	77419.309885	59.609447
2309.518327	77246.333722	59.614452
2309.211347	77064.990559	59.619457
2308.644943	76882.670003	59.624461
2307.533851	76708.205703	59.629466
2306.943593	76527.070662	59.634471
2306.142456	76351.350061	59.639476
2305.527115	76181.380030	59.644481
2305.075052	75998.821177	59.649485
2304.101547	75833.878309	59.654490
2303.820641	75659.266038	59.659495
2302.862880	75478.604147	59.664500
2301.958926	75303.225744	59.669505
2301.806085	75124.416149	59.674509
2300.968889	74947.813784	59.679514
2300.398788	74773.660520	59.684519
2299.643500	74599.107309	59.689524
2298.893470	74417.218230	59.694529
2298.508440	74244.288300	59.699533
2297.425965	74070.950960	59.704538
2297.060574	73886.382826	59.709543
2296.516753	73713.032847	59.714548
2295.600326	73532.280526	59.719553
2295.142402	73354.301632	59.724557
2294.146430	73185.443565	59.729562
2293.469820	73007.261709	59.734567
2292.821778	72833.878868	59.739572
2292.338568	72655.517443	59.744577
2291.545089	72485.841318	59.749581
2290.750351	72311.212973	59.754586
2290.432576	72140.704169	59.759591
2289.571741	71967.584343	59.764596
2288.920770	71796.801925	59.769601
2288.446686	71620.253734	59.774605
2287.656696	71450.953313	59.779610
2286.970465	71274.923275	59.784615
2286.190558	71092.860231	59.789620
2285.613589	70918.000592	59.794625
2285.324863	70739.093469	59.799629
2284.198874	70573.192068	59.804634
2284.007026	70388.609886	59.809639
2283.109836	70220.078132	59.814644
2282.377008	70037.276271	59.819649
2281.869182	69863.200462	59.824653
2280.973965	69686.711029	59.829658
2280.120844	69508.259312	59.834663
2279.361744	69349.062077	59.839668
2278.949553	69180.570011	59.844673
2278.390767	68992.581855	59.849677
2277.744947	68830.957692	59.854682
2277.617538	68643.037491	59.859687
2276.640970	68468.744404	59.864692
2275.856251	68289.716602	59.869697
2275.465359	68118.943896	59.874701
2274.164923	67935.320674	59.879706
2273.921708	67762.431300	59.884711
2273.109008	67590.868784	59.889716
2272.277687	67408.822811	59.894721
2272.044720	67233.523537	59.899725
2271.172120	67065.965100	59.904730
2270.662931	66870.940749	59.909735
2269.886358	66707.730532	59.914740
2269.186850	66525.149485	59.919745
2268.943174	66356.101026	59.924750
2268.003986	66174.606242	59.929754
2267.449116	65993.261198	59.934759
2266.243811	65816.713599	59.939764
2265.929153	65638.490683	59.944769
2265.336946	65462.545696	59.949774
2264.567043	65294.280274	59.954778
2263.977161	65107.959048	59.959783
2263.161902	64949.750407	59.964788
2262.287558	64772.457016	59.969793
2261.933589	64588.896018	59.974798
2260.974033	64415.877959	59.979802
2260.797302	64234.074798	59.984807
2259.811965	64062.058195	59.989812
2258.936271	63889.971931	59.994817
2258.601571	63711.567493	59.999822
2257.979554	63545.272779	60.004826
2257.538540	63374.398132	60.009831
2256.674949	63193.989715	60.014836
2256.199065	63016.032094	60.019841
2255.529717	62850.938180	60.024846
2254.583837	62664.776425	60.029850
2254.047594	62481.536906	60.034855
2253.062591	62309.105565	60.039860
2252.621684	62134.981287	60.044865
2252.479321	61956.689464	60.049870
2251.508444	61777.856433	60.054874
2251.059680	61604.412587	60.059879
2250.389731	61412.815576	60.064884
2249.792141	61231.430823	60.069889
2248.918774	61055.941570	60.074894
2247.842467	60878.985667	60.079898
2247.872485	60696.056706	60.084903
2247.070385	60518.718828	60.089908
2246.055073	60330.514566	60.094913
2245.640110	60163.941383	60.099918
2245.012592	59978.012084	60.104922
2243.899452	59802.620070	60.109927
2243.122561	59622.706896	60.114932
2242.694383	59445.592099	60.119937
2242.195613	59280.568926	60.124942
2241.290969	59104.504683	60.129946
2240.593131	58919.682761	60.134951
2239.984510	58741.992378	60.139956
2239.255198	58578.034356	60.144961
2238.912366	58394.585669	60.149966
2238.181624	58215.330790	60.154970
2237.773265	58038.178763	60.159975
2237.090699	57867.076020	60.164980
2236.351125	57680.003713	60.169985
2235.548856	57496.810855	60.174990
2234.735572	57320.954765	60.179994
2234.116742	57143.806700	60.184999
2233.505415	56969.649973	60.190004
2233.047713	56795.521160	60.195009
2232.694078	56606.009040	60.200014
2231.664938	56432.718030	60.205018
2231.252717	56256.466679	60.210023
2230.502958	56071.782713	60.215028
2229.942912	55888.608562	60.220033
2229.351228	55701.577183	60.225038
2228.440186	55521.016272	60.230042
2227.806188	55335.080818	60.235047
2227.123425	55150.645507	60.240052
2226.454577	54981.330085	60.245057
2225.768998	54789.943169	60.250062
2225.025664	54611.184240	60.255066
2224.532439	54430.403275	60.260071
2223.479554	54259.506782	60.265076
2223.003287	54076.134974	60.270081
2222.542610	53904.714354	60.275086
2221.617418	53715.101315	60.280090
2221.156406	53530.470018	60.285095
2220.653818	53357.042387	60.290100
2219.674317	53175.480853	60.295105
2219.086603	52996.877651	60.300110
2218.209091	52818.686058	60.305114
2217.697971	52635.742509	60.310119
2217.110027	52453.762231	60.315124
2216.259555	52279.552121	60.320129
2216.031610	52096.262200	60.325134
2214.813466	51923.784468	60.330138
2214.360608	51742.448053	60.335143
2213.836315	51557.653933	60.340148
2213.288454	51384.239765	60.345153
2212.890894	51192.759733	60.350158
2212.073261	51020.635275	60.355162
2211.299394	50822.767764	60.360167
2210.448762	50652.613648	60.365172
2209.969879	50473.926446	60.370177
2209.499688	50287.064559	60.375182
2208.328479	50118.456492	60.380186
2207.857174	49918.943817	60.385191
2207.020455	49750.213405	60.390196
2206.092680	49570.331498	60.395201
2205.929915	49391.279128	60.400206
2204.803688	49221.960599	60.405210
2204.147111	49036.764270	60.410215
2203.810332	48879.911390	60.415220
2202.994981	48693.826408	60.420225
2202.488067	48513.989654	60.425230
2201.495192	48340.460519	60.430234
2201.187157	48156.916817	60.435239
2200.604259	47986.154159	60.440244
2199.857260	47811.344857	60.445249
2199.525450	47622.654296	60.450254
2198.896611	47452.881522	60.455258
2198.100156	47271.917105	60.460263
2197.502055	47074.926962	60.465268
2196.951437	46902.078813	60.470273
2196.520783	46719.670261	60.475278
2195.318820	46530.487307	60.480282
2194.715202	46348.119534	60.485287
2194.333528	46167.628898	60.490292
2193.623867	45983.731861	60.495297
2192.939162	45803.204480	60.500302
2191.959681	45619.496398	60.505306
2191.374670	45430.803086	60.510311
2190.672953	45262.973396	60.515316
2189.947033	45080.663515	60.520321
2189.562507	44892.671652	60.525326
2188.645886	44719.824006	60.530330
2187.964969	44528.615974	60.535335
2187.298740	44361.950032	60.540340
2186.386831	44181.990964	60.545345
2186.041169	43991.282786	60.550350
2185.168774	43818.845047	60.555354
2184.715645	43632.515881	60.560359
2183.822256	43460.088199	60.565364
2183.206557	43288.642824	60.570369
2182.686939	43103.879497	60.575374
2181.864192	42932.366133	60.580378
2181.743185	42744.403133	60.585383
2180.993224	42565.551469	60.590388
2179.876953	42384.027530	60.595393
2179.280254	42208.782422	60.600398
2178.481351	42043.601824	60.605402
2178.188331	41848.658831	60.610407
2177.541156	41671.308512	60.615412
2176.301441	41488.485478	60.620417
2176.138470	41306.107027	60.625422
2175.363088	41139.008818	60.630426
2174.894809	40951.999514	60.635431
2174.020930	40775.086507	60.640436
2173.353856	40596.112525	60.645441
2172.761526	40422.415338	60.650446
2172.049297	40245.749340	60.655450
2171.627126	40069.995624	60.660455
2170.745827	39889.393546	60.665460
2170.128664	39707.809254	60.670465
2169.443159	39531.848327	60.675470
2168.757792	39356.309707	60.680474
2167.960291	39179.766288	60.685479
2167.289133	39000.801775	60.690484
2166.863776	38826.787661	60.695489
2165.975053	38642.522981	60.700494
2165.219861	38465.529738	60.705498
2164.999214	38293.858220	60.710503
2164.277438	38109.281983	60.715508
2163.861993	37931.499040	60.720513
2163.496679	37738.263145	60.725518
2162.321163	37556.333602	60.730522
2161.699955	37382.826951	60.735527
2160.787589	37200.146607	60.740532
2160.431060	37027.300278	60.745537
2159.669150	36832.477972	60.750542
2159.106681	36660.436268	60.755546
2158.636349	36471.044011	60.760551
2157.635970	36292.650372	60.765556
2157.044804	36109.842388	60.770561
2156.590053	35931.786452	60.775566
2155.826431	35742.719209	60.780570
2155.162740	35559.421373	60.785575
2154.389428	35375.072932	60.790580
2153.928928	35197.638941	60.795585
2153.403213	35008.001723	60.800590
2152.122424	34825.453081	60.805594
2151.761645	34641.010935	60.810599
2151.399851	34459.979949	60.815604
2150.340759	34284.578734	60.820609
2149.557702	34096.339204	60.825614
2149.081016	33917.269892	60.830618
2148.282330	33732.768200	60.835623
2147.636275	33549.639773	60.840628
2146.713255	33378.916949	60.845633
2146.257148	33192.386774	60.850638
2145.820011	33023.889850	60.855642
2145.378966	32839.489894	60.860647
2144.469247	32659.869161	60.865652
2143.156593	32478.361142	60.870657
2143.146560	32294.496204	60.875662
2142.409490	32128.957246	60.880666
2141.896399	31935.876659	60.885671
2140.806675	31759.633191	60.890676
2140.153112	31576.102734	60.895681
2139.729994	31401.996395	60.900686
2139.171868	31223.541153	60.905690
2138.310783	31043.898702	60.910695
2137.769649	30878.996961	60.915700
2137.094833	30686.539733	60.920705
2136.435428	30500.672663	60.925710
2135.773607	30331.567384	60.930714
2135.293781	30146.756571	60.935719
2134.211678	29966.546366	60.940724
2133.408289	29788.717603	60.945729
2132.958900	29611.434993	60.950734
2132.466137	29444.375483	60.955738
2131.742654	29254.620810	60.960743
2131.261531	29085.523451	60.965748
2130.462928	28909.831634	60.970753
2130.044031	28717.548148	60.975758
2129.220258	28546.332114	60.980762
2128.613130	28361.773413	60.985767
2127.671185	28189.417132	60.990772
2126.874224	28001.922586	60.995777
2126.487030	27822.736446	61.000782
2125.552105	27657.229898	61.005786
2124.883281	27485.122128	61.010791
2124.254755	27303.093827	61.015796
2123.233540	27134.922351	61.020801
2123.345356	26954.152493	61.025806
2122.307363	26780.240439	61.030810
2121.775041	26598.376207	61.035815
2121.081653	26425.489051	61.040820
2120.311240	26245.857538	61.045825
2120.145950	26069.061402	61.050830
2119.056507	25893.963416	61.055834
2118.585787	25706.704381	61.060839
2118.028877	25539.677942	61.065844
2116.940543	25369.167797	61.070849
2116.149895	25172.231052	61.075854
2115.580430	25012.401285	61.080858
2114.729345	24835.351616	61.085863
2114.442933	24666.893502	61.090868
2113.516343	24498.890165	61.095873
2113.163908	24320.742005	61.100878
2112.169770	24149.110882	61.105882
2112.036548	23973.008755	61.110887
2111.377029	23803.767640	61.115892
2110.372092	23620.468313	61.120897
2109.794056	23442.500788	61.125902
2108.832701	23271.743344	61.130906
2108.470293	23096.263725	61.135911
2107.999595	22917.776498	61.140916
2107.343109	22750.837661	61.145921
2106.465041	22570.504886	61.150926
2105.445723	22395.969507	61.155930
2104.853730	22229.840812	61.160935
2104.200586	22051.631532	61.165940
2103.528885	21879.103618	61.170945
2102.888625	21717.544724	61.175950
2102.306253	21541.847169	61.180954
2101.665927	21371.672764	61.185959
2101.241377	21209.345012	61.190964
2100.681876	21029.557220	61.195969
2100.210573	20842.068887	61.200974
2099.110122	20676.469088	61.205978
2098.722425	20490.114535	61.210983
2098.063252	20318.605979	61.215988
2097.259529	20146.060735	61.220993
2096.481278	19971.087205	61.225998
2095.414771	19807.099006	61.231002
2095.082785	19621.760807	61.236007
2094.247931	19463.378338	61.241012
2093.435860	19291.679875	61.246017
2092.849979	19121.381062	61.251022
2092.186334	18959.197785	61.256026
2091.526226	18794.779139	61.261031
2090.881869	18625.201167	61.266036
2089.996550	18450.448330	61.271041
2089.311818	18284.711152	61.276046
2088.741641	18130.547655	61.281050
2087.996382	17958.041746	61.286055
2087.505146	17797.730643	61.291060
2086.736662	17633.623255	61.296065
2086.334511	17457.402160	61.301070
2085.289828	17310.985529	61.306074
2084.402485	17151.834256	61.311079
2084.163228	16988.747506	61.316084
2083.184971	16830.850670	61.321089
2082.830709	16662.503121	61.326094
2082.286436	16502.803637	61.331098
2081.366378	16335.289814	61.336103
2080.507189	16184.016676	61.341108
2079.742936	16025.416283	61.346113
2079.314465	15854.836631	61.351118
2078.678984	15701.220096	61.356122
2078.206976	15537.399745	61.361127
2077.343289	15383.007368	61.366132
2076.748635	15236.735204	61.371137
2076.041116	15065.762234	61.376142
2075.095398	14900.431017	61.381146
2074.641116	14746.552065	61.386151
2073.727020	14590.045695	61.391156
2072.856275	14447.023007	61.396161
2072.141539	14288.269506	61.401166
2071.884692	14138.797929	61.406170
2071.072870	13983.803696	61.411175
2070.121814	13835.973711	61.416180
2069.152904	13690.275327	61.421185
2068.527816	13532.843869	61.426190
2067.825625	13401.870472	61.431194
2067.109256	13247.510935	61.436199
2066.732382	13109.774352	61.441204
2065.880436	12976.368088	61.446209
2065.185290	12830.381543	61.451214
2064.082189	12705.460887	61.456218
2063.346141	12567.242685	61.461223
2062.791932	12426.491832	61.466228
2061.894695	12310.646185	61.471233
2061.241260	12173.168700	61.476238
2060.037914	12058.719959	61.481242
2058.986971	11930.873981	61.486247
2058.599207	11820.899982	61.491252
2057.504652	11702.441132	61.496257
2057.039697	11582.299035	61.501262
2056.358716	11479.744969	61.506266
2055.733001	11358.895333	61.511271
2055.201589	11254.704832	61.516276
2054.084731	11137.678578	61.521281
2053.363638	11027.999153	61.526286
2052.615499	10930.639736	61.531290
2052.277254	10824.814662	61.536295
2051.454530	10720.825167	61.541300
2050.508105	10623.551468	61.546305
2050.046222	10511.262443	61.551310
2049.093286	10416.393079	61.556314
2048.231837	10313.779891	61.561319
2047.894425	10229.769385	61.566324
2046.978804	10122.630515	61.571329
2046.386360	10020.617299	61.576334
2045.474558	9943.850171	61.581338
2044.975106	9846.765593	61.586343
2044.583752	9769.102139	61.591348
2043.757619	9668.487409	61.596353
2042.985860	9568.994919	61.601358
2042.124959	9493.657539	61.606362
2041.580928	9389.364363	61.611367
2040.779945	9308.000626	61.616372
2040.154117	9221.097930	61.621377
2039.894740	9129.181430	61.626382
2038.728194	9052.135819	61.631386
2038.264195	8961.818864	61.636391
2037.344359	8878.623502	61.641396
2036.439583	8791.311562	61.646401
2035.763926	8720.124461	61.651406
2035.169843	8651.833894	61.656410
2034.738333	8569.014805	61.661415
2034.096529	8483.311367	61.666420
2033.138552	8414.334112	61.671425
2032.899599	8329.506026	61.676430
2032.050927	8256.930928	61.681434
2031.229781	8172.564148	61.686439
2030.424156	8086.498479	61.691444
2029.581707	8023.833565	61.696449
2028.984230	7950.138529	61.701454
2028.128137	7881.992064	61.706458
2027.846469	7803.332916	61.711463
2027.133406	7737.802409	61.716468
2026.440229	7663.331161	61.721473
2025.934835	7591.571785	61.726478
2025.068511	7527.743649	61.731482
2024.262361	7464.962517	61.736487
2023.855762	7386.201938	61.741492
2022.673397	7325.247344	61.746497
2022.136288	7247.982963	61.751502
2021.280860	7190.736674	61.756506
2020.944095	7130.166949	61.761511
2020.539197	7054.454746	61.766516
2019.764152	6996.921142	61.771521
2019.139608	6924.435287	61.776526
2018.362662	6869.795901	61.781530
2017.476263	6793.474377	61.786535
2016.483632	6735.451753	61.791540
2015.840697	6670.296605	61.796545
2015.436102	6608.481609	61.801550
2014.701378	6563.415984	61.806554
2014.433592	6489.940890	61.811559
2013.591611	6435.448311	61.816564
2012.966555	6387.458289	61.821569
2012.561219	6313.696687	61.826574
2011.644402	6243.654539	61.831578
2010.890190	6200.115481	61.836583
2010.416391	6133.534956	61.841588
2009.811045	6074.394903	61.846593
2009.420911	5995.682065	61.851598
2008.211736	5943.153689	61.856602
2008.121510	5870.413861	61.861607
2007.583779	5812.255611	61.866612
2006.330796	5756.358130	61.871617
2005.841412	5677.908827	61.876622
2005.343165	5631.580405	61.881626
2004.374860	5561.760255	61.886631
2003.878334	5497.882163	61.891636
2003.050817	5436.531187	61.896641
2002.323000	5386.091148	61.901646
2001.513873	5324.299177	61.906650
2001.147467	5271.971494	61.911655
2000.420834	5214.769979	61.916660
1999.432464	5161.079873	61.921665
1999.146667	5098.750685	61.926670
1998.217051	5044.509820	61.931674
1997.828861	4984.711832	61.936679
1996.897867	4927.587247	61.941684
1996.210785	4871.542576	61.946689
1995.811618	4821.534214	61.951694
1994.778882	4775.319340	61.956698
1994.355135	4707.745088	61.961703
1993.787549	4656.912997	61.966708
1992.770382	4602.081930	61.971713
1992.272327	4548.688505	61.976718
1991.570805	4498.364849	61.981722
1990.827318	4446.227714	61.986727
1990.672912	4386.045656	61.991732
1989.896829	4345.309100	61.996737
1989.217240	4284.196557	62.001742
1988.461542	4236.877832	62.006746
1987.642610	4175.748423	62.011751
1987.248168	4118.622265	62.016756
1986.396970	4078.987537	62.021761
1986.026798	4018.729234	62.026766
1985.322544	3965.123011	62.031770
1984.691284	3894.975714	62.036775
1983.909314	3845.771985	62.041780
1983.181103	3801.698810	62.046785
1982.587100	3726.816008	62.051790
1981.959405	3682.429914	62.056794
1980.991177	3628.329746	62.061799
1980.476824	3575.410903	62.066804
1979.200863	3533.543001	62.071809
1978.903429	3473.972552	62.076814
1978.363716	3441.428134	62.081818
1977.829373	3373.969047	62.086823
1977.188115	3339.581362	62.091828
1976.724246	3281.818854	62.096833
1976.359602	3227.554964	62.101838
1975.321771	3176.834970	62.106842
1974.540503	3119.801700	62.111847
1973.936621	3073.026504	62.116852
1973.241712	3017.195195	62.121857
1972.145541	2965.845623	62.126862
1971.780017	2921.653654	62.131866
1971.191266	2868.789392	62.136871
1970.452388	2827.283836	62.141876
1969.678840	2769.186085	62.146881
1969.467867	2718.778058	62.151886
1968.488627	2664.064153	62.156890
1967.916031	2606.674072	62.161895
1967.392236	2557.554353	62.166900
1966.426672	2517.019357	62.171905
1966.028516	2452.545074	62.176910
1965.160709	2423.336324	62.181914
1964.774010	2358.324398	62.186919
1964.247042	2317.768443	62.191924
1963.214953	2257.870849	62.196929
1963.049445	2211.457028	62.201934
1961.858688	2154.087988	62.206938
1961.182508	2123.534084	62.211943
1960.837610	2064.952366	62.216948
1959.949341	2023.207853	62.221953
1959.468923	1969.443304	62.226958
1958.692711	1921.708716	62.231962
1957.900081	1863.361320	62.236967
1957.332899	1816.522030	62.241972
1956.754669	1773.348262	62.246977
1956.042870	1711.488258	62.251982
1955.489737	1658.943666	62.256986
1954.560111	1621.379863	62.261991
1954.158179	1567.043685	62.266996
1953.636069	1518.569861	62.272001
1952.818506	1465.042842	62.277006
1951.974538	1429.113982	62.282010
1951.415893	1382.456886	62.287015
1950.373971	1323.911512	62.292020
1949.694079	1282.880423	62.297025
1949.239785	1236.918482	62.302030
1948.501412	1192.968351	62.307034
1948.074551	1157.753014	62.312039
1947.114501	1102.849538	62.317044
1946.394377	1054.930691	62.322049
1945.852324	1010.568310	62.327054
1945.422523	974.216850	62.332058
1944.814188	926.924105	62.337063
1943.843001	882.083012	62.342068
1943.083836	846.019130	62.347073
1942.327970	784.417660	62.352078
1942.032074	761.260736	62.357082
1940.867606	719.765675	62.362087
1940.564399	669.708177	62.367092
1939.642727	621.496320	62.372097
1939.217391	582.147294	62.377102
1938.124574	553.542592	62.382106
1937.580488	498.614803	62.387111
1936.835759	480.582182	62.392116
1936.189292	443.183073	62.397121
1936.166197	406.445201	62.402126
1935.682198	367.582311	62.407130
1934.578050	331.905636	62.412135
1933.988719	286.404958	62.417140
1932.942084	255.757682	62.422145
1932.087368	216.380041	62.427150
1931.572648	180.504520	62.432154
1930.722330	143.193741	62.437159
1929.887162	112.199394	62.442164
1928.728556	94.357536	62.447169
1928.765957	54.371951	62.452174
1927.336437	43.576265	62.457178
1926.612737	14.313238	62.462183
1925.986523	10.429409	62.467188
1924.558250	-0.344363	62.472193
1923.401901	8.343550	62.477198
1921.845212	40.272544	62.482202
1920.844686	37.645011	62.487207
1920.316593	40.151041	62.492212
1920.710986	41.367365	62.497217
1920.257948	40.348108	62.502222
1919.635241	44.267885	62.507226
1919.896121	44.194984	62.512231
1918.460286	41.858900	62.517236
1917.379211	56.722723	62.522241
1917.277701	43.554269	62.527246
1916.343841	52.648429	62.532250
1915.500485	47.266299	62.537255
1914.917394	46.598840	62.542260
1914.969617	52.633355	62.547265
1914.530807	44.403744	62.552270
1912.944498	55.988936	62.557274
1912.541481	47.696872	62.562279
1912.293709	61.912763	62.567284
1911.510577	55.584380	62.572289
1910.800606	54.202219	62.577294
1910.102633	41.494302	62.582298
1908.947951	52.813859	62.587303
1908.607173	52.953163	62.592308
1907.390104	65.440092	62.597313
1906.951412	57.689840	62.602318
1906.906945	57.083529	62.607322
1906.516744	66.127662	62.612327
1905.929360	51.478339	62.617332
1904.238910	70.354408	62.622337
1904.278515	59.396461	62.627342
1903.849074	56.940039	62.632346
1902.815513	63.474927	62.637351
1902.298089	53.029605	62.642356
1901.610218	63.051375	62.647361
1901.042267	58.205832	62.652366
1900.284339	61.715008	62.657370
1899.352789	64.986825	62.662375
1899.159279	58.646841	62.667380
1898.302376	59.006852	62.672385
1897.716073	58.333599	62.677390
1897.027104	61.959559	62.682394
1896.192312	56.847303	62.687399
1895.841888	59.197404	62.692404
1895.018030	53.712838	62.697409
1894.271187	65.374507	62.702414
1893.268517	48.239664	62.707418
1892.394333	61.142081	62.712423
1892.372056	44.972790	62.717428
1891.392242	57.962935	62.722433
1890.899211	53.569116	62.727438
1890.404304	55.757655	62.732442
1889.283749	56.069642	62.737447
1888.749941	58.075127	62.742452
1888.563569	65.839559	62.747457
1887.998817	59.339321	62.752462
1887.319225	61.899374	62.757466
1886.707566	71.082746	62.762471
1885.890327	50.670010	62.767476
1885.180177	50.375959	62.772481
1884.471103	60.905710	62.777486
1883.729461	48.586345	62.782490
1883.188662	63.706601	62.787495
1883.090113	62.897569	62.792500
1881.792977	62.591055	62.797505
1881.392506	60.535306	62.802510
1880.923349	59.856074	62.807514
1880.232536	56.441386	62.812519
1879.181787	58.781250	62.817524
1878.107989	61.202044	62.822529
1877.959562	63.773962	62.827534
1877.504339	56.314919	62.832538
1876.356159	72.498264	62.837543
1875.952973	52.174333	62.842548
1874.968311	62.099726	62.847553
1874.773153	43.993044	62.852558
1874.019217	58.470635	62.857562
1873.022099	68.618779	62.862567
1872.647327	58.780006	62.867572
1871.766624	67.436825	62.872577
1871.395271	59.269045	62.877582
1870.981320	70.213987	62.882586
1870.072775	60.081497	62.887591
1870.045067	46.548103	62.892596
1869.048123	61.452200	62.897601
1868.731216	62.907601	62.902606
1867.138485	53.880355	62.907610
1866.300398	63.363020	62.912615
1866.419620	48.759222	62.917620
1865.042190	62.679810	62.922625
1865.339146	47.623603	62.927630
1864.132191	64.014965	62.932634
1863.223874	56.716169	62.937639
1862.916471	53.125499	62.942644
1862.254268	64.371620	62.947649
1861.543992	63.825288	62.952654
1860.743253	59.708982	62.957658
1860.513166	60.332178	62.962663
1860.202830	53.726905	62.967668
1858.907505	59.084407	62.972673
1857.869386	61.196775	62.977678
1857.174909	61.015359	62.982682
1856.524076	56.939908	62.987687
1856.840767	51.782040	62.992692
1855.719378	59.983497	62.997697
1854.979504	53.927382	63.002702
1854.215261	62.400135	63.007706
1853.699130	58.979797	63.012711
1853.435259	63.514386	63.017716
1852.426335	68.742845	63.022721
1851.757519	53.368472	63.027726
1850.469073	45.931349	63.032730
1849.927658	60.305818	63.037735
1849.702753	49.992264	63.042740
1849.036882	50.086999	63.047745
1848.579611	44.006521	63.052750
1847.849880	41.307638	63.057754
1847.023619	47.355471	63.062759
1846.897808	53.044518	63.067764
1845.875023	61.924167	63.072769
1845.057681	52.609827	63.077774
1843.596425	61.939131	63.082778
1843.505563	47.035964	63.087783
1843.911002	40.525206	63.092788
1842.719428	54.421016	63.097793
1842.159870	45.929902	63.102798
1841.342036	57.304807	63.107802
1840.624767	53.824948	63.112807
1839.358181	48.264046	63.117812
1838.294530	54.434729	63.122817
1838.810192	39.559845	63.127822
1838.221031	46.079378	63.132826
1836.991230	49.524721	63.137831
1836.492915	54.049225	63.142836
1835.752188	58.150183	63.147841
1835.293258	50.294359	63.152846
1834.802751	52.952130	63.157850
1834.173627	59.694053	63.162855
1833.072211	49.103367	63.167860
1832.146099	58.492782	63.172865
1831.365212	49.437583	63.177870
1831.175001	55.042241	63.182874
1830.806579	59.396316	63.187879
1830.148539	51.494838	63.192884
1829.376330	59.793822	63.197889
1828.939411	50.972584	63.202894
1828.467366	46.222220	63.207898
1826.890478	48.719759	63.212903
1826.503998	42.500316	63.217908
1825.801574	54.593317	63.222913
1825.482821	40.327151	63.227918
1824.441769	52.853955	63.232922
1824.467920	45.455690	63.237927
1824.088485	50.347663	63.242932
1822.612888	62.446745	63.247937
1821.650415	54.864837	63.252942
1821.172334	46.854368	63.257946
1820.370355	56.785457	63.262951
1820.278856	55.314581	63.267956
1819.728491	52.938876	63.272961
1819.359230	54.254364	63.277966
1818.194546	49.492559	63.282970
1816.863088	61.653910	63.287975
1816.780578	50.921944	63.292980
1815.887661	53.724038	63.297985
1815.567728	47.503491	63.302990
1814.906400	49.668006	63.307994
1814.210829	57.062286	63.312999
1813.771785	49.665348	63.318004
1812.504967	60.996438	63.323009
1811.858830	48.874822	63.328014
1811.473953	58.952568	63.333018
1810.890449	54.584172	63.338023
1810.739027	56.823837	63.343028
1809.857858	44.993429	63.348033
1808.866691	47.427934	63.353038
1808.007514	53.304391	63.358042
1807.083767	56.869881	63.363047
1807.058521	49.583853	63.368052
1805.822314	63.767461	63.373057
1805.887938	51.920747	63.378062
1805.452519	56.488884	63.383066
1804.399704	59.067219	63.388071
1803.726663	46.711766	63.393076
1802.856260	60.935055	63.398081
1802.462572	43.965338	63.403086
1801.859922	46.270345	63.408090
1800.913306	50.333041	63.413095
1800.064218	39.752774	63.418100
1799.117187	55.038452	63.423105
1798.620141	53.486898	63.428110
1798.439636	48.182480	63.433114
1797.688654	61.902694	63.438119
1797.452791	48.416555	63.443124
1796.805529	59.876346	63.448129
1795.957319	51.114119	63.453134
1795.147474	52.029651	63.458138
1794.279997	61.277305	63.463143
1794.176099	43.786921	63.468148
1792.899477	57.797177	63.473153
1792.193116	49.982232	63.478158
1791.402075	57.271832	63.483162
1791.091483	55.641787	63.488167
1790.317848	60.825017	63.493172
1789.890201	54.933806	63.498177
1789.512118	57.294618	63.503182
1788.553371	51.874089	63.508186
1787.556123	60.637738	63.513191
1787.034977	53.990262	63.518196
1786.156923	58.193462	63.523201
1786.015325	58.026769	63.528206
1785.481729	54.703836	63.533210
1784.414383	65.217959	63.538215
1783.922864	57.859318	63.543220
1782.750812	56.619956	63.548225
1782.305161	56.895775	63.553230
1781.881607	51.681992	63.558234
1781.456484	61.908054	63.563239
1780.583793	45.597867	63.568244
1779.336467	48.989248	63.573249
1779.116561	58.020532	63.578254
1778.649732	51.840663	63.583258
1777.950885	63.225074	63.588263
1777.798117	56.361409	63.593268
1776.712894	53.624382	63.598273
1775.604919	47.435946	63.603278
1774.922457	56.406645	63.608282
1774.258902	57.879257	63.613287
1773.866129	46.488536	63.618292
1773.491170	55.997016	63.623297
1773.088610	53.842273	63.628302
1772.169791	60.858863	63.633306
1770.726041	61.592800	63.638311
1770.914809	49.715497	63.643316
1770.108826	54.326715	63.648321
1769.844406	48.109976	63.653326
1768.478714	53.125461	63.658330
1767.756861	65.860215	63.663335
1767.148496	52.171466	63.668340
1766.705439	47.970011	63.673345
1766.268307	59.669242	63.678350
1765.639847	52.184126	63.683354
1764.707744	58.877982	63.688359
1763.996873	53.137408	63.693364
1762.996320	63.439084	63.698369
1762.666490	41.302723	63.703374
1762.496062	56.870348	63.708378
1761.208056	51.869541	63.713383
1760.432277	48.112000	63.718388
1759.349069	56.827806	63.723393
1758.982079	50.587934	63.728398
1758.681521	56.873999	63.733402
1758.308049	54.861292	63.738407
1758.109621	48.187807	63.743412
1756.926713	65.587762	63.748417
1756.105858	48.080357	63.753422
1755.626530	60.954785	63.758426
1754.984163	57.824170	63.763431
1754.547186	53.173906	63.768436
1753.008140	56.171669	63.773441
1752.642305	52.560334	63.778446
1752.085223	58.275294	63.783450
1751.880025	60.629155	63.788455
1751.886283	55.373926	63.793460
1750.360932	60.671815	63.798465
1749.508263	51.006742	63.803470
1749.000727	51.314472	63.808474
1747.876115	47.656488	63.813479
1747.135993	49.056112	63.818484
1746.484779	52.548377	63.823489
1746.229898	54.332977	63.828494
1745.827793	52.849933	63.833498
1745.265462	48.527079	63.838503
1744.920836	47.630981	63.843508
1743.738908	51.276914	63.848513
1743.288519	43.374032	63.853518
1742.717764	51.830264	63.858522
1741.258141	56.553182	63.863527
1740.764236	42.469392	63.868532
1739.670945	53.632599	63.873537
1739.448437	46.179215	63.878542
1738.945043	55.187711	63.883546
1738.552456	63.563617	63.888551
1738.065803	46.589760	63.893556
1736.513515	61.840697	63.898561
1736.321188	49.702229	63.903566
1735.605005	57.823603	63.908570
1734.972034	53.029432	63.913575
1734.878802	49.295962	63.918580
1733.455946	56.878300	63.923585
1732.507814	57.093585	63.928590
1732.049778	52.749438	63.933594
1731.888232	53.669258	63.938599
1731.652466	56.996201	63.943604
1730.516886	52.136779	63.948609
1729.486240	52.436130	63.953614
1728.729731	58.294728	63.958618
1728.377328	52.457812	63.963623
1728.264868	55.482904	63.968628
1727.151366	52.651045	63.973633
1726.161191	48.866067	63.978638
1725.970538	57.216206	63.983642
1725.318853	49.756869	63.988647
1724.883834	46.634334	63.993652
1723.016575	46.325409	63.998657
1722.541049	54.230371	64.003662
1722.277441	49.407504	64.008666
1721.454534	55.213571	64.013671
1721.226492	48.106412	64.018676
1720.831703	58.028043	64.023681
1720.461464	52.514076	64.028686
1719.444669	49.968053	64.033690
1718.627045	49.658002	64.038695
1718.133399	48.981113	64.043700
1717.304281	58.017692	64.048705
1716.297567	50.177939	64.053710
1715.574271	46.850461	64.058714
1715.351587	47.182340	64.063719
1715.133267	47.740602	64.068724
1713.985418	51.726480	64.073729
1712.943983	59.853786	64.078734
1712.743806	46.604847	64.083738
1711.771396	57.707867	64.088743
1711.180569	45.791968	64.093748
1710.793627	63.138050	64.098753
1709.900759	54.447604	64.103758
1709.309870	46.989657	64.108762
1708.664034	50.056885	64.113767
1708.322892	48.993086	64.118772
1706.918955	45.721677	64.123777
1706.214451	45.696431	64.128782
1705.834534	49.930918	64.133786
1704.915366	51.921950	64.138791
1704.584211	46.928470	64.143796
1704.337524	52.573636	64.148801
1703.571081	43.848927	64.153806
1702.932083	39.703840	64.158810
1702.153019	53.221944	64.163815
1701.902679	35.814774	64.168820
1700.522992	41.896926	64.173825
1699.387976	39.674035	64.178830
1699.132012	40.741313	64.183834
1698.483369	51.240987	64.188839
1698.385657	48.116921	64.193844
1697.811648	55.559722	64.198849
1696.710352	41.438382	64.203854
1696.065359	40.208386	64.208858
1695.226318	44.585180	64.213863
1695.008528	42.522528	64.218868
1693.919215	45.707504	64.223873
1693.078866	40.276099	64.228878
1692.529380	39.187050	64.233882
1691.967373	50.235922	64.238887
1691.714764	31.944470	64.243892
1691.304568	52.280906	64.248897
1690.362527	45.563121	64.253902
1689.958244	42.650172	64.258906
1689.009197	55.263323	64.263911
1688.114224	38.163542	64.268916
1687.283184	59.079329	64.273921
1686.540068	40.637125	64.278926
1686.131386	46.891478	64.283930
1685.326462	50.630514	64.288935
1685.398399	47.168851	64.293940
1683.648541	49.395909	64.298945
1683.304987	40.268157	64.303950
1682.910000	48.163480	64.308954
1682.089319	51.564407	64.313959
1682.282175	46.372585	64.318964
1681.242967	44.643827	64.323969
1680.433245	47.614092	64.328974
1679.613228	45.058908	64.333978
1678.468678	49.459003	64.338983
1677.776073	49.644759	64.343988
1677.322746	48.381170	64.348993
1676.863131	53.539776	64.353998
1676.276821	55.514217	64.359002
1675.725109	47.334137	64.364007
1675.523968	41.843785	64.369012
1674.282369	56.611742	64.374017
1673.662044	45.506346	64.379022
1672.831475	50.299685	64.384026
1672.381250	51.195977	64.389031
1671.813764	42.701446	64.394036
1670.882183	48.299286	64.399041
1670.287418	53.801052	64.404046
1669.917012	45.015026	64.409050
1668.812460	56.047583	64.414055
1667.917930	46.553198	64.419060
1667.172252	50.793749	64.424065
1667.078925	52.245194	64.429070
1666.658945	46.496296	64.434074
1665.979365	52.514570	64.439079
1665.247029	45.255719	64.444084
1664.367990	56.446418	64.449089
1663.851525	45.890640	64.454094
1663.644222	49.142103	64.459098
1662.310005	52.148379	64.464103
1661.512354	41.343964	64.469108
1660.908671	43.018399	64.474113
1660.564061	41.169855	64.479118
1660.145788	42.806953	64.484122
1659.144379	43.089073	64.489127
1658.467662	46.066602	64.494132
1657.361092	44.756974	64.499137
1657.038978	55.442904	64.504142
1656.973940	37.034931	64.509146
1655.654119	46.286653	64.514151
1655.256963	42.049548	64.519156
1654.580167	50.147330	64.524161
1653.787903	48.026128	64.529166
1653.396997	36.190462	64.534170
1652.162034	46.789582	64.539175
1652.237257	38.946732	64.544180
1651.518509	43.520467	64.549185
1650.467126	39.456671	64.554190
1649.626292	43.852684	64.559194
1648.640161	47.819206	64.564199
1648.608513	42.207319	64.569204
1647.882150	53.996647	64.574209
1647.226215	44.831793	64.579214
1646.299930	48.866078	64.584218
1645.485768	47.685044	64.589223
1645.310252	46.309523	64.594228
1644.811322	46.573329	64.599233
1644.484245	39.346305	64.604238
1643.522466	43.129190	64.609242
1642.778632	41.042877	64.614247
1642.556170	42.456489	64.619252
1641.384792	50.058842	64.624257
1640.603856	39.586088	64.629262
1640.237650	46.303617	64.634266
1639.309377	49.691686	64.639271
1638.412837	41.665743	64.644276
1637.772285	45.919562	64.649281
1637.250142	47.223089	64.654286
1636.842999	43.905337	64.659290
1635.769423	58.723887	64.664295
1634.934172	48.581447	64.669300
1634.260103	55.179157	64.674305
1633.878101	36.149776	64.679310
1633.697650	49.109182	64.684314
1632.961014	47.379686	64.689319
1632.498153	35.929185	64.694324
1631.447012	49.733362	64.699329
1630.801617	47.082647	64.704334
1630.620772	42.626686	64.709338
1629.240426	52.629187	64.714343
1628.391053	40.956238	64.719348
1628.047108	48.783534	64.724353
1627.412351	43.084534	64.729358
1627.274668	49.655380	64.734362
1625.752434	54.760453	64.739367
1625.419577	42.070342	64.744372
1624.704582	50.483272	64.749377
1624.206938	42.698312	64.754382
1622.940508	49.798543	64.759386
1621.932546	48.607304	64.764391
1622.117788	43.025617	64.769396
1621.334910	44.356375	64.774401
1620.954922	52.151553	64.779406
1620.969590	39.119240	64.784410
1619.712278	44.872915	64.789415
1618.893329	40.617671	64.794420
1618.449707	54.758996	64.799425
1617.766656	42.782092	64.804430
1616.684925	45.946970	64.809434
1615.732640	54.891174	64.814439
1615.894457	39.440153	64.819444
1615.330740	50.432535	64.824449
1614.039152	35.513600	64.829454
1613.583504	44.292172	64.834458
1612.580486	43.789262	64.839463
1612.551785	40.559626	64.844468
1611.684060	48.150018	64.849473
1610.317982	43.027662	64.854478
1610.057919	43.097413	64.859482
1609.406036	46.698618	64.864487
1608.885998	42.488929	64.869492
1608.652718	45.465406	64.874497
1607.905326	45.324002	64.879502
1606.995441	54.718777	64.884506
1606.218149	55.790039	64.889511
1605.842849	45.982965	64.894516
1604.862870	47.304040	64.899521
1604.155614	44.771968	64.904526
1604.120895	51.905184	64.909530
1603.258902	49.025542	64.914535
1602.197155	40.095483	64.919540
1601.472681	37.581917	64.924545
1600.483777	49.988532	64.929550
1600.433508	47.762083	64.934554
1599.889257	50.474160	64.939559
1599.091767	49.908642	64.944564
1597.858251	46.613375	64.949569
1597.628343	40.780683	64.954574
1597.555116	46.633253	64.959578
1596.713331	47.981262	64.964583
1595.743873	37.806553	64.969588
1594.871232	46.171993	64.974593
1594.563099	51.415350	64.979598
1593.853709	44.119766	64.984602
1592.343741	61.002452	64.989607
1591.930323	48.758795	64.994612
1591.345133	54.542897	64.999617
1590.979303	53.429422	65.004622
1590.703413	47.720725	65.009626
1590.194341	61.162844	65.014631
1589.437423	38.958788	65.019636
1588.194036	47.022019	65.024641
1587.852135	43.824795	65.029646
1587.581557	47.467926	65.034650
1586.397632	52.415196	65.039655
1585.682674	43.061050	65.044660
1585.115076	47.074637	65.049665
1584.628416	52.672779	65.054670
1583.927689	38.539906	65.059674
1582.691807	48.970469	65.064679
1582.430290	37.035420	65.069684
1581.942319	52.088936	65.074689
1581.626166	56.483614	65.079694
1580.728860	46.455135	65.084698
1579.709886	47.504878	65.089703
1579.254239	42.786661	65.094708
1578.849253	58.815724	65.099713
1577.795695	53.907076	65.104718
1577.165567	47.753203	65.109722
1576.082866	49.757644	65.114727
1576.360334	50.916797	65.119732
1575.637893	46.767656	65.124737
1574.182720	35.575751	65.129742
1573.887857	40.654575	65.134746
1573.066640	52.663983	65.139751
1572.948269	48.683790	65.144756
1571.855588	42.880947	65.149761
1571.183799	42.755926	65.154766
1570.782464	36.519979	65.159770
1570.131589	48.808241	65.164775
1569.485590	41.291288	65.169780
1568.792950	39.241017	65.174785
1567.952641	43.583355	65.179790
1567.834973	45.376129	65.184794
1566.764296	51.005562	65.189799
1566.047447	43.428905	65.194804
1565.302700	43.971472	65.199809
1564.436687	50.651727	65.204814
1564.086195	51.866496	65.209818
1562.919672	52.482385	65.214823
1562.472151	51.060203	65.219828
1561.969209	43.567830	65.224833
1561.661330	52.259856	65.229838
1561.623771	46.322492	65.234842
1560.024123	41.880656	65.239847
1559.680400	37.824311	65.244852
1558.436311	41.762463	65.249857
1557.443348	47.735932	65.254862
1556.873031	39.896308	65.259866
1556.421626	43.145558	65.264871
1556.015326	42.014866	65.269876
1555.662472	44.355926	65.274881
1555.188309	47.941522	65.279886
1554.477516	37.487622	65.284890
1553.705712	52.419083	65.289895
1553.072812	43.178065	65.294900
1551.856113	48.550013	65.299905
1551.080454	50.715408	65.304910
1550.923959	36.846155	65.309914
1550.062820	50.557087	65.314919
1550.155457	46.056105	65.319924
1548.802761	42.682031	65.324929
1547.740377	46.523511	65.329934
1547.560492	41.400373	65.334938
1546.992419	50.091163	65.339943
1546.916051	50.183772	65.344948
1546.033403	42.502582	65.349953
1544.779508	53.410675	65.354958
1544.423661	39.839593	65.359962
1543.042371	50.692234	65.364967
1542.787040	50.611433	65.369972
1542.276011	38.094734	65.374977
1541.836107	38.270335	65.379982
1540.568565	44.456166	65.384986
1539.567413	54.336956	65.389991
1539.536991	36.973735	65.394996
1539.045872	40.256104	65.400001
1538.799125	43.323032	65.405006
1538.177186	34.342051	65.410010
1536.793615	63.644932	65.415015
1536.181679	45.730718	65.420020
1535.909746	45.367135	65.425025
1535.133684	50.760537	65.430030
1534.447284	41.378221	65.435034
1533.749547	42.968281	65.440039
1533.297487	43.596812	65.445044
1531.927044	43.767311	65.450049
1531.228246	53.814521	65.455054
1530.974531	40.143638	65.460058
1530.647975	48.677785	65.465063
1530.190007	45.856972	65.470068
1528.956753	44.329418	65.475073
1527.974553	52.316481	65.480078
1527.910951	52.328216	65.485082
1527.232920	46.459507	65.490087
1526.510030	35.307394	65.495092
1525.552368	52.081837	65.500097
1525.084167	51.132869	65.505102
1524.702492	43.250663	65.510106
1523.576464	49.436094	65.515111
1522.843951	45.443108	65.520116
1522.505272	48.161956	65.525121
1522.150717	35.826978	65.530126
1521.261183	36.955521	65.535130
1519.948156	44.052157	65.540135
1519.635938	41.454186	65.545140
1519.116582	44.168628	65.550145
1518.719984	42.780941	65.555150
1518.174460	35.486156	65.560154
1517.131046	46.321386	65.565159
1516.925572	37.195388	65.570164
1515.451069	41.324708	65.575169
1514.563352	46.592357	65.580174
1514.148007	44.453885	65.585178
1513.384900	51.507299	65.590183
1513.198405	37.223362	65.595188
1513.144302	38.372117	65.600193
1512.381222	50.358104	65.605198
1511.221755	40.317704	65.610202
1510.645346	50.687656	65.615207
1510.067070	36.576359	65.620212
1509.021235	49.930304	65.625217
1508.413098	53.139815	65.630222
1508.005075	45.520412	65.635226
1507.385454	53.101370	65.640231
1506.513985	48.107053	65.645236
1505.534046	56.629916	65.650241
1504.818974	48.701345	65.655246
1504.815635	42.462089	65.660250
1504.346286	57.014349	65.665255
1503.305377	53.037258	65.670260
1502.500124	42.103235	65.675265
1501.990118	47.506405	65.680270
1501.732608	50.220241	65.685274
1500.520320	52.068690	65.690279
1500.096503	46.069711	65.695284
1499.652231	43.133191	65.700289
1498.831457	52.643138	65.705294
1498.033600	51.025910	65.710298
1497.200338	47.816898	65.715303
1497.083562	55.174454	65.720308
1496.201851	44.692540	65.725313
1495.225518	57.792607	65.730318
1494.888440	39.566666	65.735322
1493.806629	48.635558	65.740327
1492.950816	48.599723	65.745332
1491.986350	49.339648	65.750337
1491.645152	42.334089	65.755342
1491.565774	43.310247	65.760346
1491.206939	46.891717	65.765351
1490.816595	36.148807	65.770356
1489.795427	56.412018	65.775361
1488.898704	44.540080	65.780366
1488.353403	45.774777	65.785370
1486.621647	49.128155	65.790375
1486.406092	42.313937	65.795380
1485.875061	53.594445	65.800385
1485.383462	47.338164	65.805390
1485.078675	47.252613	65.810394
1484.353462	48.643631	65.815399
1483.605601	45.255477	65.820404
1483.072746	48.145531	65.825409
1482.042130	47.432599	65.830414
1481.256683	33.363699	65.835418
1480.234595	50.161003	65.840423
1480.188316	47.542852	65.845428
1479.835719	37.993975	65.850433
1479.181958	42.256231	65.855438
1478.377580	43.861675	65.860442
1477.481562	43.445891	65.865447
1477.207937	51.407096	65.870452
1476.209792	46.864996	65.875457
1475.297096	42.572663	65.880462
1474.810653	40.350883	65.885466
1474.065927	50.288707	65.890471
1474.053180	40.928665	65.895476
1472.991187	38.833043	65.900481
1471.801171	44.547702	65.905486
1471.737430	45.429915	65.910490
1470.979064	47.512161	65.915495
1470.229933	43.674794	65.920500
1469.498251	40.711418	65.925505
1468.668238	39.045696	65.930510
1468.414103	33.636335	65.935514
1467.776166	39.446180	65.940519
1466.712906	28.792875	65.945524
1466.298326	39.983907	65.950529
1465.641768	36.168101	65.955534
1465.419017	34.101532	65.960538
1464.305934	53.043708	65.965543
1463.757885	35.007425	65.970548
1463.064611	34.713964	65.975553
1462.341827	39.425572	65.980558
1461.518710	41.026115	65.985562
1460.251469	35.448184	65.990567
1460.148622	44.085547	65.995572
1459.831124	39.763284	66.000577
1459.808129	54.001762	66.005582
1458.686201	32.428214	66.010586
1457.759344	46.662099	66.015591
1457.425652	32.756377	66.020596
1456.372327	45.021877	66.025601
1455.610208	41.747960	66.030606
1455.672747	40.563275	66.035610
1454.696141	34.647431	66.040615
1453.866945	37.461585	66.045620
1452.905304	32.470587	66.050625
1452.648582	38.470578	66.055630
1451.891017	40.737200	66.060634
1450.494792	45.196304	66.065639
1449.830534	36.408153	66.070644
1449.825090	48.254817	66.075649
1449.554434	47.454236	66.080654
1448.738209	38.106778	66.085658
1447.941060	41.436221	66.090663
1447.111369	32.030986	66.095668
1446.759676	36.133280	66.100673
1445.319404	47.222407	66.105678
1445.220082	33.162749	66.110682
1444.374425	44.870138	66.115687
1444.454539	43.729967	66.120692
1443.143216	40.650567	66.125697
1442.047210	45.774726	66.130702
1441.923925	42.588513	66.135706
1441.193934	42.252009	66.140711
1440.436347	48.989178	66.145716
1439.543423	36.189443	66.150721
1438.895821	54.981956	66.155726
1438.637962	42.270516	66.160730
1437.948428	63.799335	66.165735
1437.868101	47.645660	66.170740
1436.759037	47.180174	66.175745
1436.167250	45.948098	66.180750
1435.458842	46.458119	66.185754
1434.145259	37.006792	66.190759
1433.631621	46.428513	66.195764
1433.365407	35.222779	66.200769
1432.635194	46.459251	66.205774
1432.425785	36.665284	66.210778
1431.075681	44.127387	66.215783
1430.615316	44.195876	66.220788
1430.401752	37.600543	66.225793
1428.916182	49.956829	66.230798
1428.386522	32.811750	66.235802
1427.622605	41.800173	66.240807
1427.561906	48.030781	66.245812
1426.904556	37.628360	66.250817
1426.255830	36.498374	66.255822
1425.264076	39.579640	66.260826
1424.639153	42.719295	66.265831
1424.229899	44.167342	66.270836
1423.495907	41.349423	66.275841
1422.284001	46.130897	66.280846
1422.187957	42.019441	66.285850
1421.500130	40.611827	66.290855
1421.055203	35.948713	66.295860
1419.862145	38.879054	66.300865
1419.073951	40.677480	66.305870
1418.965493	33.666487	66.310874
1418.274630	44.948744	66.315879
1417.388590	39.926820	66.320884
1416.696733	42.179853	66.325889
1416.128029	43.323670	66.330894
1415.796402	36.370223	66.335898
1414.808475	45.551946	66.340903
1414.209724	38.264074	66.345908
1414.017887	41.590356	66.350913
1412.983784	36.391701	66.355918
1412.235330	36.966439	66.360922
1411.607280	43.072759	66.365927
1410.744239	37.386458	66.370932
1409.762741	40.603290	66.375937
1409.066493	40.882734	66.380942
1408.761568	31.335763	66.385946
1408.417588	44.366869	66.390951
1407.992790	38.423262	66.395956
1406.869970	35.589881	66.400961
1406.091446	46.419309	66.405966
1406.022595	33.999531	66.410970
1404.465144	38.425936	66.415975
1403.535819	37.714283	66.420980
1403.251296	43.794388	66.425985
1402.815872	37.228016	66.430990
1402.455279	46.298993	66.435994
1401.802975	38.977060	66.440999
1401.218429	40.645354	66.446004
1400.292098	47.215393	66.451009
1399.594340	50.475438	66.456014
1399.608020	37.066434	66.461018
1398.079507	51.097930	66.466023
1397.479292	35.593021	66.471028
1397.279672	48.266881	66.476033
1396.146687	40.497817	66.481038
1395.693009	32.470978	66.486042
1394.545871	46.787196	66.491047
1394.255335	37.816663	66.496052
1393.915758	42.369610	66.501057
1392.620529	42.299576	66.506062
1392.209264	35.771943	66.511066
1391.580474	46.856687	66.516071
1391.399694	32.857294	66.521076
1390.760838	41.212429	66.526081
1389.343895	48.841291	66.531086
1389.126031	43.897669	66.536090
1388.621340	41.254620	66.541095
1387.417408	40.616582	66.546100
1387.074057	38.507691	66.551105
1386.212101	37.610299	66.556110
1386.436855	36.819287	66.561114
1385.022666	37.241238	66.566119
1384.383282	44.580931	66.571124
1383.635083	39.420420	66.576129
1383.136347	43.289058	66.581134
1382.685804	36.158983	66.586138
1381.552488	42.098047	66.591143
1381.360862	29.667831	66.596148
1380.511788	42.176843	66.601153
1379.409748	36.724081	66.606158
1378.835114	45.221971	66.611162
1377.854255	41.612276	66.616167
1377.993868	37.086486	66.621172
1377.696775	39.964312	66.626177
1376.535383	47.574635	66.631182
1376.145798	41.759473	66.636186
1375.318778	51.909087	66.641191
1374.297117	36.978942	66.646196
1373.750550	43.293085	66.651201
1372.842324	40.070804	66.656206
1372.570930	42.477782	66.661210
1372.154666	38.034043	66.666215
1371.388727	38.149538	66.671220
1370.660773	42.111382	66.676225
1369.719875	43.773251	66.681230
1369.299013	41.348686	66.686234
1368.313305	49.528735	66.691239
1367.880603	43.966426	66.696244
1367.713986	35.841925	66.701249
1366.757692	39.158841	66.706254
1365.666882	42.281104	66.711258
1365.164830	42.589613	66.716263
1364.707233	37.556375	66.721268
1364.508516	38.387507	66.726273
1363.312591	45.158100	66.731278
1362.627245	39.814145	66.736282
1362.038465	41.325429	66.741287
1361.059446	37.587720	66.746292
1360.168459	41.857748	66.751297
1359.668139	38.952244	66.756302
1359.696610	43.435651	66.761306
1359.187560	44.459613	66.766311
1357.799235	38.358529	66.771316
1357.319592	43.201819	66.776321
1356.190197	45.992762	66.781326
1356.237980	37.335877	66.786330
1355.324231	40.177693	66.791335
1354.539669	38.266672	66.796340
1354.178672	41.317080	66.801345
1353.490745	47.393508	66.806350
1352.954596	35.565247	66.811354
1351.817170	48.099607	66.816359
1351.442169	32.694533	66.821364
1350.809134	36.847867	66.826369
1350.341419	41.635646	66.831374
1348.937463	35.790936	66.836378
1348.189566	39.145691	66.841383
1348.143248	35.415835	66.846388
1347.943250	30.165041	66.851393
1346.931057	43.980439	66.856398
1346.251516	27.483680	66.861402
1345.626471	38.787017	66.866407
1344.885808	37.408324	66.871412
1343.856963	41.148354	66.876417
1342.960388	43.511218	66.881422
1343.047854	31.763597	66.886426
1342.077100	33.067532	66.891431
1341.648978	31.230738	66.896436
1341.191946	35.997896	66.901441
1340.292230	45.006349	66.906446
1339.621877	34.479877	66.911450
1338.532554	40.013005	66.916455
1338.081395	36.519389	66.921460
1337.352307	35.643469	66.926465
1336.952455	30.053874	66.931470
1336.919562	35.128910	66.936474
1335.764127	32.368556	66.941479
1335.247734	36.590079	66.946484
1334.042459	31.871246	66.951489
1332.955444	38.933608	66.956494
1332.677782	34.835265	66.961498
1331.820394	32.489565	66.966503
1331.696810	31.766540	66.971508
1331.547767	34.899946	66.976513
1330.104282	42.123056	66.981518
1329.481958	37.633239	66.986522
1329.024685	42.206478	66.991527
1328.190353	48.977949	66.996532
1327.422142	31.826681	67.001537
1326.463406	31.824609	67.006542
1326.321990	36.429633	67.011546
1326.075818	37.334542	67.016551
1325.215546	35.080763	67.021556
1324.823308	37.227842	67.026561
1323.771652	33.599465	67.031566
1322.772291	23.897995	67.036570
1321.824285	36.203551	67.041575
1321.497685	34.379005	67.046580
1321.089904	43.353410	67.051585
1320.509781	37.595360	67.056590
1319.962747	28.198861	67.061594
1319.127794	40.953212	67.066599
1318.311507	33.491804	67.071604
1317.561592	36.435315	67.076609
1316.693997	31.099851	67.081614
1316.387404	31.214875	67.086618
1315.839014	46.833067	67.091623
1315.477196	40.740700	67.096628
1314.386976	29.323808	67.101633
1313.434304	44.446468	67.106638
1313.255373	34.007457	67.111642
1312.692091	33.775369	67.116647
1311.640689	49.738454	67.121652
1310.746673	39.242816	67.126657
1310.014524	36.405718	67.131662
1310.504147	32.680545	67.136666
1309.451292	41.573005	67.141671
1308.429153	31.209704	67.146676
1308.234528	32.781335	67.151681
1306.928493	34.182739	67.156686
1306.240325	34.781038	67.161690
1305.653081	33.087816	67.166695
1305.271480	31.598436	67.171700
1305.000968	32.247027	67.176705
1303.763740	41.011110	67.181710
1303.618646	27.669947	67.186714
1302.848441	19.327620	67.191719
1301.709721	40.639249	67.196724
1300.547118	39.269304	67.201729
1300.085924	33.814044	67.206734
1299.868052	27.238344	67.211738
1299.316223	35.768883	67.216743
1298.699964	30.978501	67.221748
1297.881869	30.159319	67.226753
1297.051302	35.848436	67.231758
1296.613299	29.361348	67.236762
1296.132746	32.184771	67.241767
1295.293485	30.608887	67.246772
1294.672534	36.673097	67.251777
1294.020101	38.380591	67.256782
1293.528556	31.220791	67.261786
1292.233781	34.364471	67.266791
1291.652737	41.343252	67.271796
1291.390861	30.807051	67.276801
1290.715173	41.121844	67.281806
1289.973229	28.495299	67.286810
1289.005590	36.178919	67.291815
1288.582684	41.563538	67.296820
1288.275109	34.582641	67.301825
1287.381315	37.616842	67.306830
1286.911950	30.973897	67.311834
1286.103098	39.805493	67.316839
1285.472281	37.950474	67.321844
1284.611551	36.775386	67.326849
1283.653507	39.274195	67.331854
1283.312996	38.831659	67.336858
1282.761731	32.972843	67.341863
1282.136110	40.621013	67.346868
1281.373500	34.587647	67.351873
1280.979655	37.496633	67.356878
1280.611562	33.616096	67.361882
1279.511421	41.987821	67.366887
1278.862840	34.868760	67.371892
1278.453211	31.338594	67.376897
1276.571402	40.435399	67.381902
1276.650722	32.295465	67.386906
1276.141785	34.850599	67.391911
1275.631075	40.712789	67.396916
1275.125793	30.298868	67.401921
1273.502420	35.822314	67.406926
1273.450338	22.275568	67.411930
1272.900812	44.827592	67.416935
1272.196830	38.657176	67.421940
1271.541565	36.139017	67.426945
1270.671325	38.351064	67.431950
1270.393331	30.610131	67.436954
1269.763562	34.712500	67.441959
1268.305391	41.611554	67.446964
1267.884875	34.795271	67.451969
1267.049144	38.665468	67.456974
1267.283856	24.973777	67.461978
1266.772049	40.603494	67.466983
1265.782632	35.673760	67.471988
1265.137759	32.329229	67.476993
1264.039244	35.946327	67.481998
1263.091110	36.038785	67.487002
1262.782235	34.213006	67.492007
1261.997201	36.914541	67.497012
1261.646043	32.856280	67.502017
1260.912604	32.368993	67.507022
1260.744915	33.505848	67.512026
1259.823695	28.172627	67.517031
1259.069676	32.857709	67.522036
1258.157633	39.660472	67.527041
1257.292141	36.045100	67.532046
1257.338436	28.977986	67.537050
1256.489142	38.005246	67.542055
1255.076271	32.247165	67.547060
1254.382222	40.905978	67.552065
1253.846832	35.956097	67.557070
1253.756666	34.273735	67.562074
1253.090068	40.386212	67.567079
1252.733751	26.211347	67.572084
1251.765206	24.509383	67.577089
1250.952554	41.267116	67.582094
1250.850165	32.705080	67.587098
1249.826475	40.845469	67.592103
1248.935649	33.561515	67.597108
1248.656013	25.898119	67.602113
1247.339595	35.829106	67.607118
1246.579162	33.606788	67.612122
1245.939344	39.467434	67.617127
1245.626768	32.775915	67.622132
1245.491213	39.775328	67.627137
1244.871140	41.130769	67.632142
1243.964150	37.941458	67.637146
1242.999271	45.027010	67.642151
1242.726890	33.823879	67.647156
1241.883437	32.277064	67.652161
1241.076638	40.255238	67.657166
1240.609792	35.612997	67.662170
1239.708572	36.734030	67.667175
1238.896469	40.996283	67.672180
1238.602680	38.699767	67.677185
1238.305775	33.691470	67.682190
1237.453867	31.367010	67.687194
1236.640096	41.892996	67.692199
1235.790761	38.164680	67.697204
1234.619921	32.150514	67.702209
1233.619711	33.392942	67.707214
1233.552895	32.903740	67.712218
1232.807809	29.226658	67.717223
1232.638551	30.934604	67.722228
1232.633957	34.672651	67.727233
1231.742676	40.019791	67.732238
1231.119883	28.861347	67.737242
1229.588326	45.353367	67.742247
1228.608246	37.834461	67.747252
1228.097253	37.576732	67.752257
1227.509040	39.715563	67.757262
1227.735197	33.931833	67.762266
1226.639338	35.832851	67.767271
1225.823600	40.762716	67.772276
1225.456028	34.458403	67.777281
1224.811754	39.785190	67.782286
1224.149978	36.325090	67.787290
1222.801459	39.494695	67.792295
1222.635922	44.256518	67.797300
1222.104248	40.058237	67.802305
1221.379825	39.856524	67.807310
1220.659335	31.843775	67.812314
1219.771913	33.937148	67.817319
1219.371480	35.943622	67.822324
1219.194525	43.763303	67.827329
1218.170837	39.245880	67.832334
1217.408060	32.766301	67.837338
1216.678033	33.659853	67.842343
1216.013738	35.933783	67.847348
1215.124818	29.813299	67.852353
1213.923631	39.694440	67.857358
1213.839155	29.431236	67.862362
1213.531812	33.505998	67.867367
1212.808407	32.449444	67.872372
1212.236241	35.771558	67.877377
1211.242653	43.331603	67.882382
1210.839325	24.365704	67.887386
1209.946047	36.047590	67.892391
1208.986520	22.996805	67.897396
1208.890529	34.521945	67.902401
1208.355519	33.599432	67.907406
1207.810053	34.897286	67.912410
1206.686901	33.175771	67.917415
1205.916001	33.525486	67.922420
1205.824655	35.538002	67.927425
1204.317834	40.989341	67.932430
1203.898937	30.159594	67.937434
1203.205914	37.033195	67.942439
1202.880304	42.806038	67.947444
1202.546375	34.552056	67.952449
1201.380076	43.766934	67.957454
1200.665377	33.952444	67.962458
1200.285473	46.435769	67.967463
1199.908629	31.366919	67.972468
1198.768053	38.182387	67.977473
1197.971607	38.287016	67.982478
1197.786918	29.993535	67.987482
1196.802212	48.409163	67.992487
1195.997047	36.347776	67.997492
1195.907278	34.122899	68.002497
1195.076065	34.285095	68.007502
1194.280097	40.509616	68.012506
1193.537747	44.158412	68.017511
1192.680914	45.381210	68.022516
1192.312164	31.706637	68.027521
1191.195613	47.426225	68.032526
1190.732366	37.589096	68.037530
1190.090784	33.507648	68.042535
1189.918180	38.507129	68.047540
1189.502764	39.811113	68.052545
1187.960603	35.287850	68.057550
1187.714930	43.861181	68.062554
1187.170066	39.415855	68.067559
1186.060978	42.031755	68.072564
1185.375401	40.235932	68.077569
1184.823341	38.656988	68.082574
1184.665209	40.317438	68.087578
1183.490210	45.600907	68.092583
1182.254154	38.750338	68.097588
1182.257626	42.036108	68.102593
1181.593785	37.680666	68.107598
1181.549418	39.135372	68.112602
1180.778484	36.654556	68.117607
1179.739492	40.896138	68.122612
1179.592591	31.741968	68.127617
1178.306769	39.659144	68.132622
1177.447743	30.105731	68.137626
1176.794410	41.446704	68.142631
1176.508587	43.382920	68.147636
1175.754530	32.713710	68.152641
1174.856794	38.487656	68.157646
1174.474623	37.173425	68.162650
1173.931599	30.638415	68.167655
1173.263978	30.213224	68.172660
1171.998202	38.811591	68.177665
1171.498079	39.741131	68.182670
1171.435374	30.592495	68.187674
1170.615663	41.417474	68.192679
1169.307426	32.648263	68.197684
1168.964579	34.935736	68.202689
1168.321620	40.525668	68.207694
1168.172005	29.929065	68.212698
1166.959375	36.713426	68.217703
1166.282443	30.633363	68.222708
1165.975393	26.374147	68.227713
1165.418380	41.705138	68.232718
1164.651511	32.583336	68.237722
1163.816550	37.472120	68.242727
1163.357267	37.250334	68.247732
1162.644301	28.827993	68.252737
1161.401483	32.509080	68.257742
1160.764662	24.517742	68.262746
1160.348948	37.553941	68.267751
1160.027944	24.735934	68.272756
1159.327982	26.976126	68.277761
1158.221608	33.251597	68.282766
1157.665874	25.640013	68.287770
1157.429886	32.002555	68.292775
1156.822129	41.302077	68.297780
1155.823051	29.921238	68.302785
1154.785098	40.304703	68.307790
1154.656640	39.777999	68.312794
1154.360411	29.688826	68.317799
1153.592283	31.236562	68.322804
1152.948913	38.177968	68.327809
1152.087386	38.846454	68.332814
1150.754466	29.977107	68.337818
1150.366441	37.633239	68.342823
1150.057088	31.964638	68.347828
1149.809478	36.763166	68.352833
1148.418263	38.860996	68.357838
1147.823099	35.330402	68.362842
1147.462683	32.123585	68.367847
1147.039563	39.105655	68.372852
1146.017780	32.517489	68.377857
1145.120837	37.384598	68.382862
1144.975938	24.634779	68.387866
1144.057502	44.123203	68.392871
1143.040271	31.291351	68.397876
1142.651057	35.828557	68.402881
1141.878624	45.855997	68.407886
1141.836046	30.998923	68.412890
1140.865109	44.629620	68.417895
1139.960244	31.213789	68.422900
1139.391597	36.470218	68.427905
1138.600137	32.636544	68.432910
1137.668829	37.641580	68.437914
1137.043714	31.275751	68.442919
1136.730975	34.496695	68.447924
1136.644806	27.496387	68.452929
1135.491254	39.907218	68.457934
1134.923323	36.678215	68.462938
1134.402821	41.450764	68.467943
1133.337859	31.712511	68.472948
1132.521705	33.155931	68.477953
1131.854664	38.967313	68.482958
1131.599957	36.615713	68.487962
1131.155701	35.454861	68.492967
1129.785178	30.629958	68.497972
1129.112196	26.892559	68.502977
1128.537297	31.165995	68.507982
1128.373434	23.654515	68.512986
1128.121836	35.791005	68.517991
1126.786238	31.952421	68.522996
1126.500890	33.945333	68.528001
1125.565974	30.922932	68.533006
1124.406167	33.759805	68.538010
1124.096516	40.394257	68.543015
1124.033989	37.203139	68.548020
1123.433074	33.881618	68.553025
1121.983110	43.069104	68.558030
1121.626982	32.230972	68.563034
1121.303657	37.927764	68.568039
1120.013117	40.818548	68.573044
1119.370823	32.129522	68.578049
1118.445857	35.149811	68.583054
1118.524745	24.442762	68.588058
1117.830612	34.885085	68.593063
1116.756676	37.082273	68.598068
1116.202660	35.790653	68.603073
1115.249073	46.308944	68.608078
1115.267826	31.388505	68.613082
1114.566544	30.404153	68.618087
1113.518664	40.204178	68.623092
1113.167520	29.276951	68.628097
1112.352050	39.150393	68.633102
1111.632887	38.045887	68.638106
1111.042834	33.204084	68.643111
1110.628286	43.458446	68.648116
1109.854780	37.433182	68.653121
1108.627608	41.651107	68.658126
1108.381195	32.987423	68.663130
1107.712677	33.166346	68.668135
1106.861674	33.793751	68.673140
1106.420395	31.959094	68.678145
1105.918888	35.347258	68.683150
1105.386172	25.369828	68.688154
1104.453641	40.613898	68.693159
1103.566288	41.882579	68.698164
1103.235213	39.579398	68.703169
1101.708671	35.761736	68.708174
1101.183663	36.411405	68.713178
1100.872236	35.292508	68.718183
1100.294242	50.623695	68.723188
1100.118735	36.051110	68.728193
1099.413478	47.395626	68.733198
1098.838778	38.558662	68.738202
1098.005825	37.915369	68.743207
1097.266265	35.027480	68.748212
1096.238374	30.832472	68.753217
1095.077631	42.891236	68.758222
1095.184332	34.584535	68.763226
1094.632993	29.987307	68.768231
1093.999681	35.720792	68.773236
1093.220686	31.965574	68.778241
1092.210124	31.266959	68.783246
1091.853036	27.573937	68.788250
1091.408803	35.239013	68.793255
1090.556753	28.322689	68.798260
1089.763973	32.487291	68.803265
1089.504106	33.739740	68.808270
1088.902042	32.389540	68.813274
1087.675004	35.451582	68.818279
1086.783123	32.605271	68.823284
1086.632241	21.594165	68.828289
1086.059132	27.138305	68.833294
1084.902728	33.371300	68.838298
1084.306313	29.061934	68.843303
1083.952364	31.163530	68.848308
1083.681905	24.347080	68.853313
1082.310730	40.414688	68.858318
1081.666261	21.058282	68.863322
1081.287049	34.219555	68.868327
1081.048408	31.802330	68.873332
1080.169308	31.934335	68.878337
1079.206484	34.547511	68.883342
1078.947475	28.341077	68.888346
1078.021689	31.161243	68.893351
1076.722250	38.870899	68.898356
1076.528230	25.788295	68.903361
1075.896099	35.427581	68.908366
1075.651641	33.173703	68.913370
1074.611501	32.933948	68.918375
1073.828168	36.537253	68.923380
1073.607612	29.014296	68.928385
1073.112338	29.329668	68.933390
1072.317090	25.629082	68.938394
1071.239464	45.095533	68.943399
1070.719003	37.177170	68.948404
1069.936563	32.036410	68.953409
1068.944021	37.708777	68.958414
1068.456044	28.228849	68.963418
1068.130468	29.480714	68.968423
1067.978232	27.360397	68.973428
1066.880437	32.887084	68.978433
1066.094854	33.160331	68.983438
1065.764549	21.785121	68.988442
1064.515775	32.105953	68.993447
1063.786562	23.716198	68.998452
1063.757986	28.527191	69.003457
1062.903983	34.112867	69.008462
1062.239648	33.242497	69.013466
1061.297312	29.133240	69.018471
1060.524648	34.631864	69.023476
1060.403149	32.976573	69.028481
1059.114937	34.446226	69.033486
1058.762910	31.878313	69.038490
1057.863047	33.987910	69.043495
1057.540086	33.790187	69.048500
1057.069398	24.783740	69.053505
1055.906349	30.317657	69.058510
1055.311642	42.174429	69.063514
1054.912458	34.970039	69.068519
1054.140624	32.459447	69.073524
1053.522122	27.171194	69.078529
1052.876629	30.612232	69.083534
1052.344959	25.553010	69.088538
1051.857868	29.052424	69.093543
1050.584656	35.758162	69.098548
1050.081639	18.233710	69.103553
1049.468880	30.875487	69.108558
1049.314781	30.373368	69.113562
1048.222854	27.853778	69.118567
1047.412653	22.901944	69.123572
1047.333755	28.484161	69.128577
1045.942615	28.331794	69.133582
1045.349007	32.401647	69.138586
1044.422805	31.244945	69.143591
1043.952868	32.925042	69.148596
1044.062191	30.487158	69.153601
1043.232170	30.237643	69.158606
1042.517087	23.501395	69.163610
1041.690906	29.202493	69.168615
1041.070679	28.471764	69.173620
1040.417332	15.443326	69.178625
1039.450551	33.753614	69.183630
1039.159531	21.725631	69.188634
1038.606258	26.590133	69.193639
1037.407045	43.232780	69.198644
1036.880100	20.590357	69.203649
1036.190418	39.755404	69.208654
1035.703882	23.942421	69.213658
1035.344955	36.252096	69.218663
1034.078221	30.281677	69.223668
1033.767127	31.365667	69.228673
1033.172134	32.665128	69.233678
1032.413821	33.979533	69.238682
1031.812836	28.901381	69.243687
1030.944480	39.833470	69.248692
1030.942853	26.092661	69.253697
1029.300231	35.449603	69.258702
1029.088861	21.543477	69.263706
1028.525811	28.912077	69.268711
1027.796819	30.996077	69.273716
1027.112303	30.650881	69.278721
1026.240357	39.643954	69.283726
1026.047577	28.508636	69.288730
1025.454574	31.791523	69.293735
1024.383254	36.071418	69.298740
1024.037309	25.662190	69.303745
1023.206529	33.551188	69.308750
1022.451282	21.026227	69.313754
1021.465708	27.795020	69.318759
1020.898502	30.373659	69.323764
1020.891985	24.041915	69.328769
1019.894251	33.170111	69.333774
1018.860151	21.946305	69.338778
1018.656459	33.543752	69.343783
1017.895357	32.403370	69.348788
1017.419826	28.469017	69.353793
1016.278098	40.557894	69.358798
1015.741722	29.857274	69.363802
1015.294909	34.998149	69.368807
1015.021695	33.182501	69.373812
1013.834549	31.852866	69.378817
1012.785326	35.572604	69.383822
1012.815736	40.091948	69.388826
1012.371851	32.770106	69.393831
1011.161547	44.295906	69.398836
1010.604071	36.526948	69.403841
1010.120182	31.687207	69.408846
1009.635677	32.734136	69.413850
1008.509347	27.774265	69.418855
1007.787766	34.255067	69.423860
1007.509061	24.082721	69.428865
1006.371198	35.388840	69.433870
1005.614742	32.877394	69.438874
1005.185222	35.369480	69.443879
1004.550353	31.097792	69.448884
1004.533908	33.006933	69.453889
1003.140537	39.369124	69.458894
1002.547170	36.551043	69.463898
1002.328013	28.942724	69.468903
1001.144868	42.127834	69.473908
1000.290926	22.238685	69.478913
999.568992	41.687978	69.483918
999.068837	33.723831	69.488922
998.941982	28.516640	69.493927
998.421089	37.753477	69.498932
997.723652	20.100708	69.503937
996.748138	32.924783	69.508942
996.146351	21.261635	69.513946
995.158402	31.296575	69.518951
994.507557	30.275848	69.523956
994.534276	26.775661	69.528961
993.397021	45.980390	69.533966
992.913156	42.435282	69.538970
992.082543	21.910088	69.543975
991.420104	37.240511	69.548980
991.105709	26.157666	69.553985
989.945515	29.450380	69.558990
989.377770	21.293576	69.563994
988.696208	37.790794	69.568999
987.960165	28.616855	69.574004
987.428225	28.681042	69.579009
986.348736	29.094113	69.584014
986.147959	26.451687	69.589018
985.754440	37.565270	69.594023
985.004666	32.524996	69.599028
984.881790	31.204233	69.604033
984.196373	29.458905	69.609038
983.080572	26.799645	69.614042
982.363572	20.357029	69.619047
981.557233	20.042267	69.624052
980.680935	29.884409	69.629057
979.650627	33.774608	69.634062
979.204076	31.895084	69.639066
979.042248	41.368098	69.644071
978.483022	37.068612	69.649076
977.419096	36.886296	69.654081
976.725478	37.110246	69.659086
976.280352	34.322201	69.664090
976.196757	37.806313	69.669095
974.977171	45.947997	69.674100
974.356818	27.934470	69.679105
973.668942	44.834811	69.684110
972.795715	37.734249	69.689114
971.628177	38.169220	69.694119
971.064895	38.825005	69.699124
970.488067	29.091170	69.704129
970.318801	37.483611	69.709134
969.977592	36.804695	69.714138
969.300469	33.116886	69.719143
968.222822	36.519475	69.724148
967.921448	29.905075	69.729153
967.054040	32.592991	69.734158
966.045457	34.019774	69.739162
965.658917	32.791425	69.744167
965.247950	29.002924	69.749172
964.709021	36.080704	69.754177
963.496154	36.051398	69.759182
963.150449	29.846163	69.764186
962.805098	28.051462	69.769191
961.663460	42.546692	69.774196
960.900200	27.845326	69.779201
960.166203	31.257890	69.784206
959.767423	33.142714	69.789210
959.354193	28.482549	69.794215
958.258474	34.655476	69.799220
957.955434	28.744642	69.804225
957.231781	33.820767	69.809230
956.219932	29.795152	69.814234
955.549754	26.817426	69.819239
954.658706	35.767824	69.824244
954.540710	31.421791	69.829249
954.310890	35.143628	69.834254
953.415973	35.128388	69.839258
952.685378	29.739734	69.844263
951.589258	33.511109	69.849268
950.748029	19.564882	69.854273
949.800160	27.483564	69.859278
949.524629	25.669871	69.864282
949.166630	20.215627	69.869287
948.622416	33.543499	69.874292
948.847413	10.902903	69.879297
947.670064	25.277652	69.884302
946.459882	23.883909	69.889306
945.976078	18.646797	69.894311
945.130403	17.672855	69.899316
944.497590	24.313000	69.904321
943.969821	25.734243	69.909326
943.089516	31.502326	69.914330
942.552187	28.251160	69.919335
941.923832	25.063363	69.924340
941.914331	22.026243	69.929345
940.193467	29.150175	69.934350
939.953736	23.815879	69.939354
939.117932	32.670758	69.944359
938.915990	34.991026	69.949364
937.734744	26.345252	69.954369
936.894241	34.303625	69.959374
936.654372	34.132119	69.964378
936.500492	24.219037	69.969383
935.342240	38.254883	69.974388
934.694991	21.710602	69.979393
934.015413	29.427330	69.984398
933.150042	24.410203	69.989402
932.115899	37.746657	69.994407
931.372800	30.459835	69.999412
931.352652	36.138356	70.004417
930.808161	32.681757	70.009422
930.499243	27.117205	70.014426
929.514583	29.177262	70.019431
928.581868	24.866265	70.024436
928.259901	33.516383	70.029441
927.335921	30.199019	70.034446
926.619264	36.048296	70.039450
926.217442	38.364104	70.044455
925.656054	30.870178	70.049460
924.864804	24.273821	70.054465
923.717476	39.214650	70.059470
923.382918	30.490917	70.064474
923.131459	34.317119	70.069479
922.024990	30.022735	70.074484
921.479170	36.054556	70.079489
921.049645	28.446612	70.084494
919.917451	39.048562	70.089498
919.089064	33.760633	70.094503
918.619933	32.398783	70.099508
918.225262	33.805159	70.104513
917.541812	31.441392	70.109518
916.791460	20.432676	70.114522
916.213596	31.164021	70.119527
915.556375	25.541362	70.124532
915.213244	34.783032	70.129537
913.690168	27.049502	70.134542
913.246879	26.736910	70.139546
912.801254	23.166818	70.144551
912.518414	33.158958	70.149556
911.754387	21.278817	70.154561
910.806230	38.696800	70.159566
910.412018	29.552069	70.164570
909.529483	19.248766	70.169575
908.558796	36.214608	70.174580
908.005308	26.753039	70.179585
907.481713	34.424453	70.184590
907.372560	26.014926	70.189594
906.331154	26.546546	70.194599
905.579579	31.699663	70.199604
905.361767	25.384206	70.204609
904.131149	36.984230	70.209614
903.498711	27.275038	70.214618
902.876540	29.206458	70.219623
902.428009	32.564146	70.224628
901.698609	33.815642	70.229633
900.888810	32.050709	70.234638
900.547309	27.752867	70.239642
899.457421	33.841312	70.244647
898.548906	37.054592	70.249652
898.275083	25.394476	70.254657
897.447995	28.227379	70.259662
897.018876	28.771945	70.264666
896.769217	20.056789	70.269671
895.690473	29.081221	70.274676
895.184675	29.016692	70.279681
894.393077	25.689313	70.284686
893.392745	25.935290	70.289690
892.956669	19.738148	70.294695
892.076859	35.760737	70.299700
892.106945	25.894076	70.304705
891.356607	28.673767	70.309710
890.449402	28.130667	70.314714
889.719076	36.443667	70.319719
889.043981	24.111003	70.324724
888.129290	32.462803	70.329729
887.133678	31.806044	70.334734
886.603249	31.414288	70.339738
886.941169	27.244857	70.344743
886.069414	32.355606	70.349748
885.610755	23.334679	70.354753
884.626466	30.887029	70.359758
883.311655	40.568762	70.364762
882.441675	22.634433	70.369767
881.458479	35.363569	70.374772
882.038141	30.709401	70.379777
881.264124	16.925974	70.384782
880.893793	29.814603	70.389786
880.706197	22.270669	70.394791
879.246389	29.871892	70.399796
878.797448	19.755055	70.404801
877.624917	38.247927	70.409806
877.140784	24.613895	70.414810
876.541537	21.653289	70.419815
875.939771	31.164770	70.424820
875.072870	28.410757	70.429825
873.956478	34.803041	70.434830
873.661811	20.200606	70.439834
873.212142	26.663389	70.444839
872.663984	29.735749	70.449844
872.645279	23.353918	70.454849
871.256893	23.584395	70.459854
870.670323	37.292741	70.464858
869.698612	27.186564	70.469863
869.104722	21.102850	70.474868
868.417258	32.611709	70.479873
867.828527	24.281669	70.484878
867.674057	31.449654	70.489882
866.446864	19.220640	70.494887
865.438173	30.591395	70.499892
865.477435	24.733329	70.504897
864.633741	17.192900	70.509902
864.062948	27.429554	70.514906
863.385077	20.734756	70.519911
862.786333	22.665609	70.524916
862.293006	23.043787	70.529921
861.226111	21.942662	70.534926
860.746075	15.165921	70.539930
860.216574	25.263542	70.544935
859.376841	20.420555	70.549940
858.854529	19.633289	70.554945
858.520320	19.894683	70.559950
857.372117	22.176329	70.564954
856.463092	22.264291	70.569959
856.047620	20.862377	70.574964
855.536810	23.055194	70.579969
854.484852	19.789769	70.584974
853.753974	24.288343	70.589978
853.495190	16.549173	70.594983
852.771999	23.000299	70.599988
852.478619	21.965294	70.604993
851.250923	37.890302	70.609998
850.566852	25.860268	70.615002
849.789629	30.184879	70.620007
849.664999	28.001841	70.625012
848.516507	20.331738	70.630017
847.807135	24.418475	70.635022
847.356920	16.392818	70.640026
847.079845	21.560308	70.645031
846.341922	35.557662	70.650036
845.337823	24.133637	70.655041
844.896646	24.665938	70.660046
844.494849	27.308168	70.665050
843.470893	20.045587	70.670055
842.400727	32.156237	70.675060
842.270255	15.361024	70.680065
841.596054	29.217348	70.685070
841.036855	24.501598	70.690074
840.393745	20.910917	70.695079
839.726300	34.428716	70.700084
838.784323	20.378735	70.705089
837.849929	24.501289	70.710094
837.145324	25.154365	70.715098
837.103452	27.319854	70.720103
836.428907	19.498633	70.725108
835.671299	18.933320	70.730113
834.490746	20.488445	70.735118
834.325876	21.232226	70.740122
833.831486	23.378280	70.745127
832.710060	32.967750	70.750132
832.401909	14.846265	70.755137
831.718264	30.731984	70.760142
831.127430	19.653762	70.765146
829.962565	19.736724	70.770151
829.196284	15.071287	70.775156
829.164415	15.674055	70.780161
828.448017	19.440227	70.785166
827.539205	20.734491	70.790170
826.875414	30.046123	70.795175
826.213245	34.432849	70.800180
825.940552	19.435860	70.805185
824.888634	27.577713	70.810190
824.194803	19.422109	70.815194
823.861654	26.853488	70.820199
823.136770	17.578501	70.825204
822.274867	19.499212	70.830209
821.480833	23.597854	70.835214
821.187955	21.905207	70.840218
820.730042	19.502418	70.845223
819.832259	25.164510	70.850228
819.167830	20.675243	70.855233
818.204122	16.301422	70.860238
817.417782	24.836227	70.865242
816.977457	18.038982	70.870247
816.367234	31.497212	70.875252
815.953424	21.587681	70.880257
815.499710	23.966952	70.885262
814.122396	26.220434	70.890266
813.783328	26.599297	70.895271
813.158303	15.565949	70.900276
812.996670	23.797897	70.905281
811.455736	15.840213	70.910286
811.010567	20.118283	70.915290
810.650010	18.482141	70.920295
809.554129	26.712995	70.925300
808.987519	18.606530	70.930305
808.143070	22.628047	70.935310
807.894002	28.710413	70.940314
807.697040	23.780900	70.945319
806.301004	29.817187	70.950324
806.007533	21.662513	70.955329
805.436478	25.254175	70.960334
804.519567	22.996988	70.965338
803.901213	22.920433	70.970343
803.033640	22.501940	70.975348
802.823858	18.479608	70.980353
801.793599	23.718107	70.985358
800.861679	23.242050	70.990362
800.567102	14.311725	70.995367
799.947897	21.727138	71.000372
799.366460	23.795594	71.005377
798.016248	21.052316	71.010382
797.408225	30.068081	71.015386
797.180467	27.360587	71.020391
796.212329	41.050836	71.025396
796.479644	24.334224	71.030401
795.435513	34.608392	71.035406
794.386037	27.056590	71.040410
794.289302	23.443602	71.045415
793.589162	31.261398	71.050420
792.888001	24.576638	71.055425
791.824944	28.986185	71.060430
791.284965	28.810428	71.065434
790.658097	19.494619	71.070439
789.764701	24.985717	71.075444
789.608571	15.039910	71.080449
788.752214	16.291145	71.085454
787.581266	31.082806	71.090458
787.320713	18.810351	71.095463
786.613396	32.616766	71.100468
786.438211	18.203488	71.105473
785.160753	22.743356	71.110478
784.140050	28.525948	71.115482
783.996969	21.047481	71.120487
783.575475	34.048335	71.125492
782.952719	17.322037	71.130497
782.170269	23.978147	71.135502
781.413559	29.922136	71.140506
781.060420	18.402409	71.145511
780.022713	22.825269	71.150516
779.334303	16.687247	71.155521
778.448859	18.887677	71.160526
778.292145	23.430482	71.165530
777.934125	11.909961	71.170535
776.627251	20.388868	71.175540
776.331994	12.570369	71.180545
775.649311	17.540664	71.185550
774.637934	25.354392	71.190554
774.377174	18.374037	71.195559
773.622076	20.706678	71.200564
772.934886	16.473354	71.205569
771.604949	11.810938	71.210574
771.217769	17.333412	71.215578
771.193558	13.762498	71.220583
770.377968	20.103775	71.225588
769.511590	18.201244	71.230593
768.530254	18.846355	71.235598
768.356493	20.834149	71.240602
768.005182	21.415233	71.245607
766.550379	22.033219	71.250612
766.151451	20.680725	71.255617
765.706798	15.757536	71.260622
765.067000	18.806657	71.265626
764.549038	20.005607	71.270631
763.646457	29.796794	71.275636
762.975461	15.921331	71.280641
761.866111	21.681771	71.285646
761.341947	27.358517	71.290650
760.611776	13.024140	71.295655
760.353149	28.782281	71.300660
760.237368	17.022931	71.305665
759.158225	17.795575	71.310670
758.394697	29.326018	71.315674
757.499780	22.626386	71.320679
756.412776	24.231307	71.325684
756.184169	29.086747	71.330689
755.794309	21.450458	71.335694
755.448539	27.265956	71.340698
754.486069	22.940847	71.345703
753.651282	33.826650	71.350708
753.103873	14.272037	71.355713
752.388851	26.439706	71.360718
751.374174	22.231716	71.365722
750.865682	17.804376	71.370727
750.330525	29.090314	71.375732
749.974553	15.814386	71.380737
748.672267	17.751615	71.385742
747.847826	19.190164	71.390746
747.967685	23.274216	71.395751
747.346934	25.987585	71.400756
746.648252	22.085669	71.405761
745.597132	21.305346	71.410766
745.110031	16.601800	71.415770
744.766206	20.745478	71.420775
743.462144	24.215736	71.425780
742.928875	25.276784	71.430785
742.490764	17.965138	71.435790
742.022796	15.153975	71.440794
741.140588	16.524454	71.445799
740.543810	28.640188	71.450804
740.285306	13.404435	71.455809
739.153172	20.635023	71.460814
738.101877	27.616210	71.465818
737.789876	26.778142	71.470823
737.267936	25.522505	71.475828
736.800878	15.186255	71.480833
735.652697	25.787648	71.485838
735.392039	23.706697	71.490842
734.639719	20.926612	71.495847
733.345482	23.236293	71.500852
733.149148	23.694941	71.505857
732.570869	17.711283	71.510862
732.168010	17.529477	71.515866
730.866105	16.680282	71.520871
729.947227	20.639557	71.525876
729.914056	17.077955	71.530881
729.264501	26.524524	71.535886
728.734164	24.462855	71.540890
727.998079	20.595284	71.545895
727.000534	30.209218	71.550900
727.036851	18.882958	71.555905
726.027840	21.192961	71.560910
725.365212	25.786353	71.565914
725.086084	22.093603	71.570919
724.062062	29.887286	71.575924
723.055759	26.892183	71.580929
722.447292	22.275770	71.585934
721.951302	23.761380	71.590938
721.522492	17.274552	71.595943
719.857535	27.240741	71.600948
719.521410	16.112547	71.605953
719.285690	19.496298	71.610958
718.772435	26.174218	71.615962
718.611774	19.520122	71.620967
717.341537	20.261710	71.625972
716.957644	22.271924	71.630977
716.054834	20.543941	71.635982
715.242503	23.685196	71.640986
714.471637	22.019782	71.645991
713.871771	24.179496	71.650996
713.748377	24.019428	71.656001
712.762514	27.200929	71.661006
711.686448	18.948534	71.666010
711.501448	15.860521	71.671015
711.017826	28.289389	71.676020
710.275839	21.168052	71.681025
709.096900	24.405524	71.686030
708.636636	33.547583	71.691034
708.558070	22.250651	71.696039
707.047284	32.138690	71.701044
706.574922	29.999988	71.706049
706.020304	29.069670	71.711054
705.705742	19.883933	71.716058
704.943530	20.000612	71.721063
703.664229	26.030977	71.726068
703.552944	21.114644	71.731073
703.040964	22.248002	71.736078
702.224571	30.426510	71.741082
701.649831	26.689370	71.746087
700.492698	34.026457	71.751092
700.539449	34.036412	71.756097
699.645225	24.403668	71.761102
698.604291	21.087674	71.766106
698.238493	22.912090	71.771111
697.480124	30.846405	71.776116
696.666081	24.408302	71.781121
695.782593	23.230740	71.786126
695.537769	26.895054	71.791130
695.363587	22.258385	71.796135
694.255066	22.666741	71.801140
693.493668	21.647930	71.806145
692.928027	22.692065	71.811150
692.263051	29.856178	71.816154
691.574857	21.603533	71.821159
690.960156	31.585436	71.826164
690.755487	22.552508	71.831169
689.743206	17.886866	71.836174
688.590747	29.403557	71.841178
688.147784	24.778147	71.846183
687.284183	30.576758	71.851188
687.260164	20.568930	71.856193
686.079663	12.904017	71.861198
685.396103	29.764255	71.866202
685.327840	25.091799	71.871207
684.395969	29.463153	71.876212
683.730092	28.183139	71.881217
683.322028	27.470757	71.886222
682.364306	25.371498	71.891226
681.642770	25.759240	71.896231
680.569914	30.298119	71.901236
680.244290	19.453678	71.906241
679.935815	33.221831	71.911246
679.324907	27.664411	71.916250
678.269162	21.113420	71.921255
677.304208	18.922279	71.926260
677.426542	15.457340	71.931265
676.614090	24.068869	71.936270
675.362426	28.118999	71.941274
674.945913	26.673130	71.946279
674.635131	26.678515	71.951284
674.154995	24.153143	71.956289
673.032754	22.168391	71.961294
672.223901	21.664903	71.966298
671.996084	28.005653	71.971303
670.518552	21.444560	71.976308
670.179894	20.514555	71.981313
669.755088	21.786997	71.986318
669.105947	22.406057	71.991322
668.629345	26.894149	71.996327
667.733826	25.716936	72.001332
667.056451	21.005860	72.006337
666.331500	29.160355	72.011342
665.886626	27.542391	72.016346
665.246526	16.957759	72.021351
664.147249	28.412375	72.026356
663.906771	19.410386	72.031361
663.446035	35.669047	72.036366
662.423479	28.374789	72.041370
661.945443	19.032173	72.046375
660.994304	29.398799	72.051380
660.783061	20.526191	72.056385
659.778601	26.561695	72.061390
658.870937	26.602205	72.066394
658.487640	16.856589	72.071399
658.070435	25.174960	72.076404
657.766685	23.222302	72.081409
656.577301	25.707705	72.086414
656.005322	26.719743	72.091418
655.575324	17.419941	72.096423
654.315291	31.978257	72.101428
653.654618	19.337479	72.106433
653.383538	25.885384	72.111438
652.632363	30.702620	72.116442
651.867749	16.408465	72.121447
650.782790	23.606345	72.126452
650.689143	17.942916	72.131457
650.655994	25.482644	72.136462
649.571618	20.708656	72.141466
649.195883	30.389170	72.146471
647.925577	23.591672	72.151476
646.929796	21.556834	72.156481
646.623714	17.005829	72.161486
645.994641	20.696641	72.166490
645.540168	26.322884	72.171495
644.570549	21.686736	72.176500
643.757299	14.534199	72.181505
643.392239	29.036728	72.186510
642.916150	32.886102	72.191514
641.969401	10.897333	72.196519
640.930959	20.520952	72.201524
640.681737	21.129950	72.206529
640.328355	30.286529	72.211534
639.640707	21.614363	72.216538
638.958399	19.658915	72.221543
638.014349	26.932130	72.226548
637.334143	31.674993	72.231553
636.289561	24.748520	72.236558
635.860952	24.544023	72.241562
635.689797	17.907380	72.246567
635.007024	24.088776	72.251572
634.050551	21.853725	72.256577
633.312809	17.582767	72.261582
632.398218	20.989479	72.266586
632.539631	14.460751	72.271591
631.576387	27.446953	72.276596
630.628249	21.254151	72.281601
630.081233	25.318239	72.286606
629.797276	32.945217	72.291610
628.914570	25.081524	72.296615
627.895604	25.084578	72.301620
627.693479	28.382565	72.306625
626.862152	35.207344	72.311630
626.030352	29.188394	72.316634
625.294736	24.229572	72.321639
624.651974	31.543119	72.326644
624.283669	20.202460	72.331649
624.074274	23.422759	72.336654
623.001868	20.573841	72.341658
622.318480	17.916853	72.346663
621.626090	27.671447	72.351668
620.649461	15.415304	72.356673
619.925104	31.681251	72.361678
619.414287	29.067740	72.366682
619.003324	19.476344	72.371687
618.412279	33.582797	72.376692
617.695039	26.747699	72.381697
617.310805	23.536888	72.386702
616.488081	33.457317	72.391706
615.637631	29.891835	72.396711
614.557337	37.864824	72.401716
613.978999	29.047526	72.406721
613.674877	27.809266	72.411726
613.059235	33.584179	72.416730
612.640044	27.855904	72.421735
611.597220	25.959454	72.426740
611.212860	18.032178	72.431745
610.410669	17.866681	72.436750
609.437040	28.325208	72.441754
609.226528	18.471666	72.446759
608.145285	21.792967	72.451764
607.389790	17.502768	72.456769
606.829386	30.894738	72.461774
606.565216	28.347601	72.466778
606.147107	27.177956	72.471783
605.077693	23.713581	72.476788
604.412347	18.524389	72.481793
603.976907	17.724920	72.486798
602.888761	25.401124	72.491802
602.113596	26.294151	72.496807
601.375816	17.415528	72.501812
600.991811	22.560638	72.506817
600.997924	26.126648	72.511822
600.155682	11.507430	72.516826
599.708532	21.071585	72.521831
598.119381	29.447301	72.526836
597.387993	25.716215	72.531841
596.548120	21.108309	72.536846
596.339189	32.321808	72.541850
596.322438	21.201124	72.546855
595.389733	26.534543	72.551860
594.608279	17.290732	72.556865
594.094850	22.481684	72.561870
593.005056	22.910756	72.566874
592.254468	17.482841	72.571879
591.079361	36.211153	72.576884
590.985677	18.337850	72.581889
590.490711	21.471172	72.586894
590.096169	22.898072	72.591898
589.768654	12.791947	72.596903
588.603453	25.176411	72.601908
588.096387	12.128017	72.606913
587.045728	23.625370	72.611918
586.006278	20.618263	72.616922
585.758348	18.191542	72.621927
585.429440	28.709814	72.626932
584.872169	10.361597	72.631937
583.601730	15.789804	72.636942
583.246315	20.853094	72.641946
582.987060	14.629445	72.646951
582.068628	25.607445	72.651956
581.145229	23.155844	72.656961
580.505207	15.538944	72.661966
580.115847	17.791312	72.666970
579.711628	15.428906	72.671975
578.427456	19.544177	72.676980
577.978196	12.683766	72.681985
577.381929	14.010337	72.686990
576.296133	22.152934	72.691994
575.785430	13.454191	72.696999
575.279520	27.089783	72.702004
575.423651	21.287569	72.707009
574.096030	17.313999	72.712014
573.059210	35.134076	72.717018
572.772124	16.857937	72.722023
572.289229	22.764669	72.727028
571.233422	16.355664	72.732033
570.492619	28.346126	72.737038
570.035057	24.240289	72.742042
569.716954	24.609538	72.747047
568.353575	26.815200	72.752052
568.100433	12.606775	72.757057
567.647668	24.672779	72.762062
566.993188	14.401123	72.767066
565.965621	20.750985	72.772071
565.299418	23.321827	72.777076
565.161445	18.334069	72.782081
564.089211	22.104944	72.787086
562.841171	14.852963	72.792090
562.386427	20.080303	72.797095
561.950655	23.688308	72.802100
561.731086	17.811564	72.807105
561.056646	21.798191	72.812110
559.954808	10.061902	72.817114
559.593984	24.647325	72.822119
559.126303	26.068534	72.827124
558.156345	20.427998	72.832129
557.360105	20.357761	72.837134
556.608114	23.524143	72.842138
556.630116	0.545391	72.847143
555.723258	30.010599	72.852148
554.934955	9.307049	72.857153
554.407621	21.000166	72.862158
553.425689	15.061932	72.867162
552.672978	14.421814	72.872167
551.874887	20.902279	72.877172
551.728131	10.751605	72.882177
551.321073	18.986365	72.887182
550.041929	20.825395	72.892186
549.680289	15.729768	72.897191
548.925800	23.978871	72.902196
548.311165	26.210357	72.907201
547.201356	19.313243	72.912206
546.651691	20.507824	72.917210
546.377390	21.164977	72.922215
545.943988	22.493999	72.927220
545.131613	19.859156	72.932225
544.494036	18.662980	72.937230
543.634893	21.565746	72.942234
542.903171	11.396288	72.947239
541.747701	19.512148	72.952244
541.271842	9.995769	72.957249
541.305139	17.979046	72.962254
540.786063	16.008666	72.967258
540.098482	11.712405	72.972263
539.193606	26.013919	72.977268
538.241686	22.849393	72.982273
537.417391	19.855343	72.987278
536.738606	17.050997	72.992282
536.285615	20.989741	72.997287
535.677281	16.226713	73.002292
534.816668	23.909273	73.007297
534.104008	13.282636	73.012302
533.678581	24.776606	73.017306
533.539500	17.819491	73.022311
532.168222	25.154480	73.027316
531.342294	19.762240	73.032321
530.711503	24.407370	73.037326
530.605741	23.673668	73.042330
530.414481	20.591402	73.047335
529.337541	18.355084	73.052340
528.354626	24.046591	73.057345
528.066518	17.330826	73.062350
526.939049	28.819937	73.067354
526.286566	18.292519	73.072359
525.748715	21.437414	73.077364
525.304276	24.799233	73.082369
524.630404	22.039837	73.087374
523.856555	25.323246	73.092378
523.730938	7.842974	73.097383
522.493626	30.513968	73.102388
521.752238	22.840694	73.107393
521.137049	15.008556	73.112398
520.553390	16.102905	73.117402
519.756049	15.575557	73.122407
518.550205	11.574739	73.127412
518.092594	20.140817	73.132417
517.905956	18.710398	73.137422
517.488301	23.435116	73.142426
517.031314	16.270033	73.147431
515.829261	26.282441	73.152436
515.416753	25.684332	73.157441
514.689957	19.379057	73.162446
513.552260	31.744978	73.167450
513.360798	10.519037	73.172455
512.588169	26.841564	73.177460
511.983286	18.247723	73.182465
510.752102	25.634520	73.187470
510.121176	22.004151	73.192474
510.210684	17.519459	73.197479
509.854129	19.673573	73.202484
509.066597	24.097681	73.207489
508.060913	16.450748	73.212494
507.353224	18.228728	73.217498
506.338355	22.051986	73.222503
505.551635	16.651936	73.227508
505.306904	23.162532	73.232513
504.979628	22.874110	73.237518
503.817129	21.182845	73.242522
502.935796	28.526531	73.247527
502.323160	24.352377	73.252532
502.133752	24.686941	73.257537
501.788157	21.358038	73.262542
500.750520	27.701644	73.267546
500.220972	17.189346	73.272551
499.568557	20.314649	73.277556
498.737454	21.837914	73.282561
497.792087	21.504457	73.287566
497.132754	26.502635	73.292570
496.777508	9.473670	73.297575
496.060742	23.863491	73.302580
495.279190	21.815090	73.307585
494.639099	21.092395	73.312590
494.013407	24.434209	73.317594
493.929545	16.441747	73.322599
492.854467	27.849985	73.327604
492.020268	19.338411	73.332609
491.755059	19.945238	73.337614
490.502686	26.446053	73.342618
489.900114	14.504114	73.347623
489.186941	22.273580	73.352628
488.790729	20.520172	73.357633
488.363886	20.820025	73.362638
487.470864	20.151818	73.367642
487.157583	12.279481	73.372647
485.997730	27.763295	73.377652
485.745042	24.201982	73.382657
484.628802	25.376452	73.387662
483.703527	32.951064	73.392666
483.518216	23.421523	73.397671
483.227439	31.987841	73.402676
482.018680	24.280231	73.407681
481.669192	25.696815	73.412686
480.854593	25.793524	73.417690
480.351933	23.949847	73.422695
479.244425	29.211807	73.427700
478.646056	24.532358	73.432705
478.502086	13.983873	73.437710
478.161116	30.849475	73.442714
477.074535	16.751768	73.447719
476.073827	30.270659	73.452724
475.786574	27.361379	73.457729
474.755432	20.472270	73.462734
474.017061	17.257983	73.467738
473.483265	7.184753	73.472743
473.093397	16.835979	73.477748
472.202262	19.624019	73.482753
471.368404	26.810345	73.487758
470.617583	31.398921	73.492762
470.362257	23.255585	73.497767
469.891375	29.999326	73.502772
469.044078	23.073045	73.507777
468.449123	25.610484	73.512782
467.744987	27.252298	73.517786
467.094692	23.710179	73.522791
466.156368	25.365649	73.527796
465.615810	23.122751	73.532801
465.109247	18.655755	73.537806
463.935241	26.301533	73.542810
463.327103	19.280387	73.547815
462.726272	22.137295	73.552820
462.498246	28.093322	73.557825
462.397790	13.242458	73.562830
461.471453	23.890599	73.567834
460.981507	10.286035	73.572839
459.789938	27.351798	73.577844
458.858961	20.416778	73.582849
458.202771	20.943978	73.587854
457.407260	24.368045	73.592858
457.412806	23.851571	73.597863
456.387247	21.039420	73.602868
455.506368	20.774550	73.607873
455.068958	13.839746	73.612878
454.350122	28.005988	73.617882
454.319118	12.648918	73.622887
453.343741	27.464710	73.627892
452.760071	24.098054	73.632897
451.825197	20.680124	73.637902
450.802257	23.820318	73.642906
450.296271	22.261018	73.647911
449.666896	26.570062	73.652916
449.688655	22.430464	73.657921
448.778606	13.459506	73.662926
447.686278	24.451051	73.667930
447.477737	19.400435	73.672935
446.366592	24.426452	73.677940
445.603835	14.053827	73.682945
445.106101	20.962687	73.687950
444.339124	24.385366	73.692954
444.169325	21.003235	73.697959
442.927501	22.049504	73.702964
442.264836	14.029422	73.707969
441.975935	18.654789	73.712974
441.299134	30.827457	73.717978
440.990944	19.105126	73.722983
439.972236	24.581601	73.727988
439.548420	20.531918	73.732993
438.900020	19.253920	73.737998
437.611368	21.116597	73.743002
437.253621	21.673521	73.748007
436.564433	24.319016	73.753012
436.008607	19.523998	73.758017
435.136632	18.291084	73.763022
434.244143	18.587868	73.768026
434.142968	24.569413	73.773031
433.614237	25.543072	73.778036
432.710160	26.168119	73.783041
431.905623	20.094447	73.788046
431.413358	31.110240	73.793050
430.959678	10.765010	73.798055
429.444824	26.611316	73.803060
428.983349	19.319242	73.808065
429.222165	23.784841	73.813070
427.988513	26.209594	73.818074
427.262455	20.744715	73.823079
426.285527	25.891276	73.828084
426.100323	26.179447	73.833089
425.892132	29.271836	73.838094
424.680747	25.103220	73.843098
424.141461	23.651729	73.848103
423.471022	27.551022	73.853108
422.717656	16.697534	73.858113
422.043550	21.239204	73.863118
421.238551	23.352822	73.868122
421.053294	15.110030	73.873127
420.053911	30.948329	73.878132
419.149434	10.149826	73.883137
418.778914	12.892777	73.888142
418.409559	8.946384	73.893146
417.957023	18.957668	73.898151
416.682963	16.260821	73.903156
416.213870	14.419695	73.908161
415.699610	16.975824	73.913166
414.185634	20.668914	73.918170
413.908772	4.682432	73.923175
413.175562	15.096389	73.928180
412.988787	22.718921	73.933185
412.905426	12.816778	73.938190
411.556689	16.196546	73.943194
411.285244	16.641956	73.948199
409.883953	14.698638	73.953204
409.201550	18.363306	73.958209
408.641361	17.889667	73.963214
408.061353	26.514683	73.968218
408.039697	13.024747	73.973223
407.020766	14.294127	73.978228
405.830716	15.004172	73.983233
405.392597	20.476454	73.988238
404.957569	15.110286	73.993242
404.607223	5.818370	73.998247
403.538866	13.053109	74.003252
402.738579	20.513210	74.008257
402.291700	14.644328	74.013262
401.537084	19.414864	74.018266
400.858664	9.719500	74.023271
400.366867	26.355246	74.028276
399.693188	20.568230	74.033281
399.376463	10.845195	74.038286
398.360122	27.993437	74.043290
398.152054	10.031188	74.048295
396.807114	28.818140	74.053300
395.739300	21.780378	74.058305
395.365536	19.685956	74.063310
394.776044	29.222352	74.068314
394.859434	11.729303	74.073319
394.207636	23.319270	74.078324
392.928680	20.996938	74.083329
392.837570	16.700294	74.088334
391.244774	28.159520	74.093338
390.749384	17.045751	74.098343
390.139595	27.812200	74.103348
389.723210	20.134498	74.108353
389.522322	25.792900	74.113358
388.452227	25.993427	74.118362
387.658268	32.619931	74.123367
386.992256	28.859575	74.128372
386.682852	21.634739	74.133377
385.690396	27.365660	74.138382
384.937954	24.057454	74.143386
384.850096	27.155901	74.148391
383.651238	23.042079	74.153396
382.787152	33.771787	74.158401
382.288304	19.326601	74.163406
381.654428	29.710553	74.168410
381.652268	26.090411	74.173415
380.590950	14.320958	74.178420
379.706848	29.549562	74.183425
379.426101	24.488383	74.188430
378.378151	28.195540	74.193434
377.703623	22.634161	74.198439
376.982100	19.335223	74.203444
376.470553	25.396352	74.208449
376.316493	15.537016	74.213454
375.091331	30.465169	74.218458
374.554387	19.615058	74.223463
374.271497	20.278329	74.228468
373.132713	26.245451	74.233473
372.419162	15.830323	74.238478
371.495608	30.590573	74.243482
371.471323	16.172270	74.248487
370.767091	22.429676	74.253492
369.773164	21.949472	74.258497
369.451517	9.945471	74.263502
368.719111	18.279396	74.268506
367.895596	15.696853	74.273511
366.883773	15.279424	74.278516
366.505962	20.672717	74.283521
366.170937	9.251144	74.288526
365.031701	14.778386	74.293530
364.604757	24.449723	74.298535
363.877081	17.039245	74.303540
363.164345	17.775745	74.308545
362.992896	13.359449	74.313550
361.702683	24.855622	74.318554
361.361114	14.753368	74.323559
361.020596	20.292100	74.328564
360.396187	20.177198	74.333569
359.223678	12.178472	74.338574
358.555783	17.643222	74.343578
358.112370	14.135976	74.348583
357.119606	19.423848	74.353588
356.531309	18.785973	74.358593
355.979323	16.070282	74.363598
355.339723	29.159512	74.368602
355.233012	11.610035	74.373607
353.817765	25.554543	74.378612
353.381167	20.363671	74.383617
352.856699	15.364992	74.388622
351.828564	21.372834	74.393626
351.429198	15.173130	74.398631
351.021065	24.721626	74.403636
350.349615	22.094356	74.408641
349.632808	15.568363	74.413646
348.707776	20.495376	74.418650
348.269746	15.038241	74.423655
347.370137	24.543639	74.428660
346.233936	24.485071	74.433665
345.956099	11.428616	74.438670
345.479044	28.186590	74.443674
345.245977	7.613861	74.448679
343.929525	17.277144	74.453684
343.193060	24.586747	74.458689
342.852745	5.272126	74.463694
342.531510	22.285946	74.468698
341.615921	15.443143	74.473703
341.099915	23.542325	74.478708
340.419684	25.678660	74.483713
339.617723	12.861844	74.488718
338.569194	24.076669	74.493722
338.335901	11.251228	74.498727
337.805152	18.321473	74.503732
336.377046	24.951281	74.508737
336.079825	17.912165	74.513742
335.313683	18.557841	74.518746
335.151683	12.189432	74.523751
334.188302	21.219314	74.528756
332.969882	12.977194	74.533761
333.076894	2.723045	74.538766
332.454076	12.704701	74.543770
332.029132	14.579587	74.548775
331.012511	9.539506	74.553780
330.247118	20.171490	74.558785
330.061715	16.041260	74.563790
328.517258	10.779383	74.568794
328.153929	15.315697	74.573799
327.212776	12.896991	74.578804
326.901214	15.310450	74.583809
326.643216	16.565822	74.588814
325.653206	13.114158	74.593818
324.908008	20.270619	74.598823
324.377122	14.090306	74.603828
323.838972	11.536414	74.608833
323.078174	18.961856	74.613838
322.297899	15.290694	74.618842
321.952279	13.943975	74.623847
320.853132	19.606768	74.628852
319.849618	20.681346	74.633857
319.678249	12.538858	74.638862
319.034265	17.764849	74.643866
318.655010	18.165951	74.648871
317.771685	11.915659	74.653876
317.155894	21.202372	74.658881
316.824326	12.121937	74.663886
315.876623	19.749049	74.668890
315.278793	15.373905	74.673895
314.554400	15.708594	74.678900
313.714088	12.012312	74.683905
312.968373	10.208988	74.688910
312.303713	8.662393	74.693914
311.965674	5.713930	74.698919
310.992397	17.684708	74.703924
310.229235	14.036053	74.708929
310.116949	17.300811	74.713934
309.210334	16.891869	74.718938
308.714601	3.076985	74.723943
307.487530	19.375767	74.728948
306.809928	9.177282	74.733953
306.704129	17.384545	74.738958
305.898477	15.393664	74.743962
305.296782	13.252011	74.748967
304.739844	18.363211	74.753972
304.223478	14.918065	74.758977
303.344092	12.689788	74.763982
302.003509	12.782081	74.768986
301.771472	15.383132	74.773991
301.282065	16.637544	74.778996
300.468662	26.439862	74.784001
299.883304	5.735650	74.789006
298.968344	15.614070	74.794010
298.727277	10.986536	74.799015
297.922590	11.299336	74.804020
297.266582	16.445249	74.809025
296.856471	10.781837	74.814030
296.080852	13.827479	74.819034
294.974394	16.126370	74.824039
294.359166	11.184749	74.829044
293.678078	22.366253	74.834049
293.619630	11.753712	74.839054
292.768721	14.473901	74.844058
291.936769	22.929361	74.849063
291.473411	19.221889	74.854068
290.791046	20.057644	74.859073
289.729770	22.868133	74.864078
288.960799	17.132612	74.869082
288.555718	7.579799	74.874087
288.312703	18.235759	74.879092
287.563608	20.540771	74.884097
286.501093	10.502986	74.889102
285.544174	15.196990	74.894106
285.337130	15.652647	74.899111
284.812881	14.424288	74.904116
284.117043	17.269568	74.909121
283.783615	12.365034	74.914126
282.930182	21.464135	74.919130
281.791517	13.672937	74.924135
281.059726	19.341845	74.929140
280.487803	16.553660	74.934145
280.357109	16.989264	74.939150
279.721783	21.688781	74.944154
278.491049	18.105201	74.949159
277.956546	20.150517	74.954164
277.493224	21.385006	74.959169
277.079103	16.969553	74.964174
275.744693	14.263480	74.969178
275.755646	9.236251	74.974183
275.087801	23.870604	74.979188
274.169397	23.233329	74.984193
273.523901	22.472133	74.989198
272.902002	15.487935	74.994202
272.657190	17.838724	74.999207
271.654329	18.477997	75.004212
271.043010	16.391500	75.009217
270.103265	8.764140	75.014222
268.919788	19.828611	75.019226
268.749946	18.088046	75.024231
267.940894	22.829448	75.029236
267.444465	28.762033	75.034241
267.306699	10.407009	75.039246
266.092044	28.152992	75.044250
265.603027	11.793525	75.049255
264.788110	20.530115	75.054260
264.200327	27.117477	75.059265
263.615912	22.454790	75.064270
262.727419	25.824351	75.069274
262.466225	24.730678	75.074279
261.944907	26.578362	75.079284
260.918717	19.633379	75.084289
260.283602	21.693159	75.089294
259.725970	28.141681	75.094298
259.098134	9.339672	75.099303
258.308594	21.511406	75.104308
257.571025	20.140443	75.109313
257.094023	26.218159	75.114318
255.994408	13.721629	75.119322
255.345394	18.426485	75.124327
255.012184	10.842793	75.129332
254.296032	22.561302	75.134337
254.191506	11.680157	75.139342
252.911751	17.538913	75.144346
252.374207	12.047204	75.149351
251.656171	18.032456	75.154356
250.317490	13.578312	75.159361
249.843481	13.929876	75.164366
249.063682	17.575415	75.169370
248.825698	18.256771	75.174375
248.723091	13.083648	75.179380
248.171026	18.550457	75.184385
247.584356	17.412477	75.189390
246.597799	18.236811	75.194394
245.827307	17.648505	75.199399
245.057773	13.155678	75.204404
244.447000	21.498625	75.209409
244.052458	15.865856	75.214414
243.086882	19.380168	75.219418
242.515716	4.624891	75.224423
241.934285	7.887164	75.229428
241.144688	14.148740	75.234433
240.187293	5.298969	75.239438
239.300076	26.652713	75.244442
239.065709	7.120973	75.249447
238.357489	16.791419	75.254452
238.175658	23.435493	75.259457
237.534242	14.298816	75.264462
236.670305	17.625047	75.269466
236.060603	7.185543	75.274471
234.794551	8.535383	75.279476
234.067333	11.358870	75.284481
233.879456	8.723936	75.289486
233.369749	7.909568	75.294490
232.580624	11.074070	75.299495
232.007441	9.282691	75.304500
231.329705	18.326988	75.309505
230.502918	19.540581	75.314510
229.404785	17.435508	75.319514
228.768692	10.138213	75.324519
228.660396	16.068848	75.329524
228.064618	17.794372	75.334529
227.695888	10.022391	75.339534
226.584549	21.813363	75.344538
226.020197	10.371615	75.349543
225.552124	17.849759	75.354548
223.957228	26.915694	75.359553
223.824624	15.572267	75.364558
223.210961	25.981401	75.369562
222.788011	16.757864	75.374567
222.010660	14.475508	75.379572
221.144039	28.170198	75.384577
220.678597	14.471926	75.389582
220.036203	25.393396	75.394586
219.375296	11.491331	75.399591
218.281781	24.665548	75.404596
217.495547	22.354647	75.409601
217.460636	16.718168	75.414606
216.960917	25.461292	75.419610
216.378591	24.100286	75.424615
215.504461	17.255660	75.429620
214.511813	22.753290	75.434625
214.092366	15.643802	75.439630
212.893523	22.462617	75.444634
212.411901	28.405464	75.449639
212.231570	25.452372	75.454644
211.844841	33.951995	75.459649
210.947708	15.279660	75.464654
210.151988	21.259961	75.469658
209.903912	21.353175	75.474663
208.288318	19.027842	75.479668
207.660561	29.995868	75.484673
207.307314	12.378499	75.489678
206.950035	18.087064	75.494682
206.548398	18.457060	75.499687
205.494695	16.966208	75.504692
204.767655	24.681175	75.509697
204.458055	14.720515	75.514702
202.937519	28.316037	75.519706
202.344115	19.242675	75.524711
202.160297	21.593207	75.529716
201.706299	20.167594	75.534721
201.104593	17.533982	75.539726
200.237434	23.642365	75.544730
199.786288	16.678277	75.549735
198.805307	20.661818	75.554740
197.911599	20.296589	75.559745
197.445518	10.151154	75.564750
196.794026	31.339603	75.569754
196.519089	21.758174	75.574759
195.312749	14.359419	75.579764
194.657515	26.478219	75.584769
194.230453	10.099443	75.589774
193.567191	30.701590	75.594778
193.151725	20.120744	75.599783
192.414480	23.729555	75.604788
191.709940	12.217131	75.609793
191.017394	25.570273	75.614798
189.960955	19.806504	75.619802
189.623778	20.945207	75.624807
189.304485	13.431846	75.629812
188.242558	25.839402	75.634817
187.688196	14.266768	75.639822
186.779820	26.405427	75.644826
186.473440	20.236664	75.649831
185.341223	26.071933	75.654836
184.310634	35.304962	75.659841
184.434051	25.841366	75.664846
183.961369	25.770126	75.669850
183.481389	12.173531	75.674855
182.409584	16.259862	75.679860
181.720749	26.521721	75.684865
181.152857	21.966806	75.689870
180.062751	27.994052	75.694874
179.452735	19.659751	75.699879
179.001810	22.303594	75.704884
178.617449	21.215375	75.709889
177.788007	13.428550	75.714894
176.920312	24.269256	75.719898
176.255021	19.800832	75.724903
176.169033	25.187041	75.729908
174.763965	24.135403	75.734913
174.423632	11.677135	75.739918
173.821122	21.513662	75.744922
172.991466	19.014166	75.749927
172.013205	20.408039	75.754932
171.364849	35.800944	75.759937
171.150307	24.533660	75.764942
170.616560	32.236743	75.769946
170.283802	13.234768	75.774951
169.473660	21.768778	75.779956
168.744163	17.526627	75.784961
167.886476	16.980632	75.789966
166.314965	27.316993	75.794970
166.168809	23.078026	75.799975
166.014240	22.982879	75.804980
165.517676	18.632631	75.809985
164.891835	15.941378	75.814990
163.383774	30.990397	75.819994
163.234524	11.777826	75.824999
162.793599	11.646336	75.830004
161.539806	24.988044	75.835009
161.094257	19.579457	75.840014
160.344754	28.510642	75.845018
160.242183	22.162739	75.850023
159.275375	14.951308	75.855028
158.171507	18.749462	75.860033
158.127530	20.729208	75.865038
157.305372	30.373692	75.870042
156.537474	14.355183	75.875047
156.050404	17.801117	75.880052
155.186346	23.346071	75.885057
154.852021	14.154154	75.890062
153.809047	25.303498	75.895066
153.241073	13.682586	75.900071
152.782157	24.882305	75.905076
151.570421	21.352531	75.910081
151.147376	20.000838	75.915086
150.217941	28.780948	75.920090
150.124777	10.650645	75.925095
149.806214	23.073722	75.930100
148.752145	26.512295	75.935105
148.451493	25.320852	75.940110
147.478153	28.137878	75.945114
146.334751	23.157515	75.950119
145.535805	17.409482	75.955124
145.185897	22.031981	75.960129
145.091554	16.756629	75.965134
143.844419	23.952164	75.970138
143.054440	32.907154	75.975143
142.552814	20.381568	75.980148
142.119874	31.608688	75.985153
141.949476	23.584334	75.990158
140.760204	27.955908	75.995162
139.927099	19.937877	76.000167
139.605924	25.293779	76.005172
138.613877	34.430793	76.010177
137.915822	14.763282	76.015182
137.176518	17.043121	76.020186
136.896012	21.009609	76.025191
136.772452	15.767301	76.030196
135.128486	27.066091	76.035201
134.815630	16.148797	76.040206
134.042736	30.022518	76.045210
133.070320	20.539700	76.050215
132.459972	16.729552	76.055220
131.613289	26.906206	76.060225
131.632205	14.717081	76.065230
131.355107	23.367949	76.070234
130.245782	22.270759	76.075239
129.308111	11.801586	76.080244
128.474338	22.110214	76.085249
128.504475	15.039444	76.090254
127.355273	16.640355	76.095258
126.569747	21.455312	76.100263
126.240627	14.320406	76.105268
125.646380	24.256545	76.110273
124.903100	15.462565	76.115278
124.059118	16.704164	76.120282
123.625387	12.015918	76.125287
123.190298	13.074051	76.130292
121.773687	16.852703	76.135297
121.367963	17.666469	76.140302
120.719312	22.819133	76.145306
120.204954	13.742660	76.150311
119.964862	13.054053	76.155316
118.787463	16.939637	76.160321
118.194981	13.194451	76.165326
117.471180	19.186961	76.170330
117.200700	16.625131	76.175335
116.388004	17.234144	76.180340
115.502194	16.810918	76.185345
115.327587	10.302631	76.190350
114.464379	21.107943	76.195354
113.248526	15.751239	76.200359
112.948725	17.081103	76.205364
112.125528	29.953643	76.210369
112.536895	17.851743	76.215374
111.043194	16.962503	76.220378
110.219374	16.051600	76.225383
109.729853	5.039493	76.230388
108.536736	21.820183	76.235393
108.060653	12.572039	76.240398
107.434682	24.009700	76.245402
106.984670	13.355548	76.250407
106.423956	18.076317	76.255412
105.428250	24.536371	76.260417
105.436069	7.041234	76.265422
104.638381	25.565982	76.270426
103.883500	8.728604	76.275431
103.307699	11.755052	76.280436
102.756081	22.376645	76.285441
102.023263	10.214363	76.290446
100.895828	17.274137	76.295450
100.440900	7.959550	76.300455
100.129227	13.807499	76.305460
99.207564	18.727746	76.310465
98.330772	4.816012	76.315470
97.612039	13.122578	76.320474
97.003499	22.796082	76.325479
96.267246	9.743411	76.330484
95.445737	15.302094	76.335489
95.022323	17.239849	76.340494
94.826893	22.667160	76.345498
93.868183	14.976674	76.350503
93.133473	10.670730	76.355508
92.714714	25.224385	76.360513
92.086039	12.611855	76.365518
90.539749	14.356525	76.370522
89.962211	23.790131	76.375527
89.971801	17.126322	76.380532
89.144898	13.716557	76.385537
88.965906	18.821139	76.390542
87.587350	14.639944	76.395546
87.232444	20.926857	76.400551
87.287302	12.013502	76.405556
85.804340	8.802973	76.410561
85.457059	19.513402	76.415566
84.305495	15.436353	76.420570
83.856048	15.104395	76.425575
83.104247	17.124480	76.430580
82.231656	10.525663	76.435585
81.871666	7.337899	76.440590
81.604039	5.480487	76.445594
80.874062	22.362364	76.450599
80.212623	7.883307	76.455604
79.016758	14.490397	76.460609
78.903435	11.022034	76.465614
77.740745	14.061657	76.470618
77.221540	10.129765	76.475623
76.671198	12.839936	76.480628
76.308151	21.677967	76.485633
75.398249	13.945016	76.490638
74.503149	23.102851	76.495642
73.731158	15.258024	76.500647
73.539833	10.827587	76.505652
72.272590	18.806914	76.510657
71.786986	5.761593	76.515662
71.182967	14.906119	76.520666
70.625702	9.718792	76.525671
70.547169	16.195008	76.530676
69.121401	11.368525	76.535681
68.784809	7.178866	76.540686
68.543251	13.767808	76.545690
67.420325	10.744290	76.550695
66.539369	4.695572	76.555700
65.901580	17.139591	76.560705
65.472483	14.320802	76.565710
64.725120	13.460796	76.570714
64.032153	10.028106	76.575719
63.623635	15.345902	76.580724
62.912050	26.619036	76.585729
62.578051	19.752989	76.590734
61.453161	16.097457	76.595738
60.678030	19.269239	76.600743
60.364779	10.452438	76.605748
59.036693	13.778632	76.610753
58.711072	8.972241	76.615758
58.000338	11.627573	76.620762
57.601099	16.423519	76.625767
56.690610	8.550330	76.630772
55.867452	15.752397	76.635777
55.806800	6.203065	76.640782
55.192301	14.141373	76.645786
54.365971	16.337347	76.650791
53.539308	17.819047	76.655796
52.996579	25.112008	76.660801
52.335995	16.923007	76.665806
50.988464	16.674362	76.670810
50.362048	15.683113	76.675815
50.274632	12.300502	76.680820
49.658310	20.582866	76.685825
49.560584	10.716183	76.690830
48.330109	19.831319	76.695834
47.587116	13.725911	76.700839
47.079741	15.386917	76.705844
45.668463	14.784181	76.710849
45.447006	21.683721	76.715854
45.183656	20.828527	76.720858
44.525638	17.409190	76.725863
43.718601	16.265408	76.730868
42.746289	17.472309	76.735873
42.689747	11.530227	76.740878
41.255604	23.538314	76.745882
40.487039	20.625442	76.750887
40.025534	21.599497	76.755892
39.548722	21.207260	76.760897
39.080546	7.731834	76.765902
38.566620	19.367663	76.770906
37.961367	22.014064	76.775911
37.544812	16.298123	76.780916
36.176361	16.048092	76.785921
35.497258	16.399292	76.790926
34.982463	20.776875	76.795930
34.504042	17.937574	76.800935
33.964061	15.045017	76.805940
32.632091	28.345629	76.810945
32.174405	11.295311	76.815950
31.374647	13.974311	76.820954
31.057989	20.251973	76.825959
31.026196	13.659422	76.830964
29.292044	17.474577	76.835969
29.182276	17.282410	76.840974
28.605178	19.086998	76.845978
27.739741	15.708633	76.850983
27.071899	17.483541	76.855988
26.137284	21.929660	76.860993
25.916172	13.620118	76.865998
25.387220	18.630712	76.871002
24.538851	18.893800	76.876007
24.281116	9.595089	76.881012
23.359109	10.931163	76.886017
22.627281	7.771178	76.891022
22.035127	14.013934	76.896026
21.292592	11.126880	76.901031
20.304865	7.700218	76.906036
19.468811	16.367697	76.911041
19.166714	12.905794	76.916046
18.498784	19.791392	76.921050
17.826718	12.075725	76.926055
16.946206	12.001758	76.931060
16.494160	15.959346	76.936065
16.432739	8.833806	76.941070
15.075788	6.227670	76.946074
14.478431	14.265748	76.951079
13.875262	7.784833	76.956084
13.406169	14.257110	76.961089
12.578596	7.687413	76.966094
11.563854	20.735588	76.971098
10.962930	21.924266	76.976103
10.830754	9.049663	76.981108
9.722231	16.877550	76.986113
9.344479	15.122862	76.991118
8.849629	23.813194	76.996122
8.122128	10.538403	77.001127
7.356937	18.771980	77.006132
6.230935	16.294584	77.011137
6.016201	10.652113	77.016142
5.631762	12.906925	77.021147
4.750773	18.590233	77.026151
3.868764	11.095707	77.031156
3.456833	16.954924	77.036161