Mon Mar 08 18:28:53 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.455806	105.621564	0.000000
-0.987176	79.949430	0.005005
-1.458804	48.471181	0.010010
-3.599951	2.879706	0.015014
-7.385974	-36.337295	0.020019
-12.864982	-25.530608	0.025024
-18.153109	-22.493663	0.030029
-22.565597	-26.337526	0.035034
-26.766458	-30.246674	0.040038
-30.552586	-25.320500	0.045043
-33.987636	-32.994372	0.050048
-37.840978	-22.869542	0.055053
-41.426830	-28.811593	0.060058
-44.777625	-17.666253	0.065062
-49.122454	-24.483813	0.070067
-52.578672	-25.113529	0.075072
-57.024649	-20.630809	0.080077
-60.281863	-27.957716	0.085082
-63.706983	-39.673080	0.090086
-67.448836	-30.264552	0.095091
-71.341558	-30.144975	0.100096
-75.266020	-11.205038	0.105101
-78.756266	-41.431979	0.110106
-82.835815	-31.326193	0.115110
-86.603567	-13.745280	0.120115
-90.123792	-28.756881	0.125120
-93.965855	-29.531553	0.130125
-97.443993	-30.722230	0.135130
-101.873938	-35.944500	0.140134
-105.596450	-17.383659	0.145139
-109.104235	-24.702060	0.150144
-113.082729	-32.571373	0.155149
-116.615334	-28.964363	0.160154
-120.352629	-14.351212	0.165158
-124.111697	-26.684962	0.170163
-127.779547	-28.658994	0.175168
-131.298191	-23.524622	0.180173
-135.320798	-23.619174	0.185178
-139.180000	-27.062266	0.190182
-142.824751	-26.600535	0.195187
-146.733676	-35.304017	0.200192
-151.215857	-23.825070	0.205197
-154.349521	-36.971296	0.210202
-157.970941	-31.976600	0.215206
-161.790329	-24.832567	0.220211
-165.640321	-23.872876	0.225216
-169.646805	-22.262188	0.230221
-173.403516	-23.741025	0.235226
-177.181577	-25.809353	0.240230
-181.021402	-23.624451	0.245235
-184.453931	-24.188377	0.250240
-188.322327	-27.423351	0.255245
-191.701715	-21.174189	0.260250
-195.376764	-25.283633	0.265254
-199.617354	-43.895201	0.270259
-203.227483	-22.225233	0.275264
-207.069541	-24.068847	0.280269
-210.647300	-37.648721	0.285274
-214.479148	-33.791980	0.290278
-218.038557	-34.419182	0.295283
-221.730934	-31.975488	0.300288
-226.100830	-22.482268	0.305293
-229.831573	-27.738617	0.310298
-233.562298	-26.730047	0.315302
-237.421897	-33.717723	0.320307
-240.660790	-22.730340	0.325312
-244.266677	-21.691217	0.330317
-248.186644	-35.981199	0.335322
-251.837209	-26.968576	0.340326
-255.482349	-24.795707	0.345331
-259.450438	-30.594416	0.350336
-263.668452	-26.313283	0.355341
-267.490664	-33.453525	0.360346
-271.176198	-38.015312	0.365350
-275.077494	-19.326370	0.370355
-278.354380	-36.325511	0.375360
-281.899230	-37.972024	0.380365
-285.771515	-35.799124	0.385370
-289.743978	-24.983162	0.390374
-293.405114	-16.553806	0.395379
-297.188558	-25.978772	0.400384
-301.327852	-27.645485	0.405389
-304.813886	-41.514218	0.410394
-308.779397	-21.974509	0.415398
-312.259756	-22.090670	0.420403
-315.811232	-23.308744	0.425408
-319.484847	-32.815852	0.430413
-323.581602	-36.621244	0.435418
-327.599058	-35.470569	0.440422
-331.261148	-42.336655	0.445427
-334.895641	-24.735690	0.450432
-338.842300	-12.769494	0.455437
-342.018286	-33.252190	0.460442
-346.061546	-23.970172	0.465446
-349.868464	-35.887482	0.470451
-353.742865	-33.539104	0.475456
-357.446675	-28.710728	0.480461
-360.715153	-29.557620	0.485466
-365.147199	-30.187211	0.490470
-368.754679	-30.033849	0.495475
-372.622298	-32.204255	0.500480
-376.632374	-25.228141	0.505485
-379.955246	-31.055540	0.510490
-383.881168	-23.939892	0.515494
-387.377600	-27.227618	0.520499
-391.383368	-39.548322	0.525504
-395.331675	-24.913725	0.530509
-398.753783	-22.847210	0.535514
-402.535943	-19.729774	0.540518
-406.291310	-26.445245	0.545523
-409.996451	-27.099354	0.550528
-414.116377	-8.561364	0.555533
-417.696965	-36.057912	0.560538
-421.183127	-35.155907	0.565542
-425.221586	-18.368630	0.570547
-428.932869	-33.361782	0.575552
-433.162096	-6.138257	0.580557
-436.450811	-34.583350	0.585562
-440.220664	-16.620019	0.590566
-443.643519	-49.537730	0.595571
-447.636836	-5.873586	0.600576
-451.730305	-15.810160	0.605581
-455.380996	-24.797190	0.610586
-459.038425	-9.961364	0.615590
-462.826887	-43.538148	0.620595
-466.447869	-10.206738	0.625600
-470.652589	-34.151756	0.630605
-473.812628	-53.044128	0.635610
-478.205449	-8.114585	0.640614
-481.434760	-26.954919	0.645619
-485.218133	-15.862935	0.650624
-489.031308	-14.484430	0.655629
-492.681676	-29.685889	0.660634
-496.334484	-28.802891	0.665638
-500.818146	-16.282362	0.670643
-504.044358	-35.282408	0.675648
-508.017982	-25.960796	0.680653
-511.719865	-19.759043	0.685658
-515.265822	-20.984008	0.690662
-519.222040	-32.617001	0.695667
-522.879307	-29.941929	0.700672
-526.694471	-16.512620	0.705677
-530.630713	-35.867551	0.710682
-534.500280	-6.902118	0.715686
-538.296251	-26.919661	0.720691
-541.623470	-21.028427	0.725696
-545.749209	-19.071658	0.730701
-549.165669	-26.813951	0.735706
-552.931680	-29.217899	0.740710
-556.607696	-22.343736	0.745715
-560.374790	-32.552991	0.750720
-564.711072	-23.588079	0.755725
-568.133872	-33.175838	0.760730
-571.963301	-29.088703	0.765734
-575.877143	-32.594883	0.770739
-579.457017	-31.062700	0.775744
-583.167514	-19.673151	0.780749
-586.561440	-20.928601	0.785754
-590.491828	-17.017685	0.790758
-594.980832	-32.953857	0.795763
-597.986394	-24.606714	0.800768
-602.049015	-14.099119	0.805773
-605.434010	-31.791652	0.810778
-609.748107	-18.684622	0.815782
-613.640602	-21.008347	0.820787
-616.963167	-22.858594	0.825792
-621.019580	-17.175597	0.830797
-624.387655	-26.749941	0.835802
-628.344520	-16.383773	0.840806
-631.918260	-30.461892	0.845811
-635.546975	-22.175991	0.850816
-639.860712	-19.066298	0.855821
-643.169505	-27.308169	0.860826
-647.462717	-26.809878	0.865830
-651.007994	-23.345149	0.870835
-654.585396	-21.136773	0.875840
-658.624670	-2.964509	0.880845
-661.970593	-25.046893	0.885850
-666.217023	-16.302726	0.890854
-669.739503	-22.160889	0.895859
-673.069191	-24.430941	0.900864
-677.227481	-15.555766	0.905869
-680.857107	-18.586818	0.910874
-684.619043	-20.038779	0.915878
-688.425747	-30.424406	0.920883
-692.032659	-25.866462	0.925888
-696.090084	-12.581110	0.930893
-699.896214	-34.302893	0.935898
-703.844178	-25.317793	0.940902
-707.413566	-26.891941	0.945907
-710.744524	-33.064474	0.950912
-714.941705	-25.658973	0.955917
-718.442817	-32.540701	0.960922
-722.523030	-16.411738	0.965926
-726.019225	-26.763346	0.970931
-729.533006	-35.959444	0.975936
-733.778251	-35.353552	0.980941
-737.347746	-33.045399	0.985946
-741.486486	-24.969563	0.990950
-744.900521	-29.629173	0.995955
-748.571732	-38.725968	1.000960
-752.569932	-12.355720	1.005965
-755.887752	-34.193280	1.010970
-759.914401	-24.172132	1.015974
-763.856252	-20.399446	1.020979
-767.119143	-32.262638	1.025984
-771.459891	-14.399985	1.030989
-775.122022	-25.103445	1.035994
-779.138977	-28.843523	1.040998
-782.789501	-32.389859	1.046003
-786.229515	-53.345267	1.051008
-790.168729	-21.820192	1.056013
-793.650662	-33.862787	1.061018
-797.735306	-39.077416	1.066022
-801.412749	-37.623920	1.071027
-804.782892	-34.350953	1.076032
-809.112941	-19.765097	1.081037
-812.433203	-30.762815	1.086042
-816.421892	-25.516076	1.091046
-820.075645	-32.294405	1.096051
-823.458776	-31.766229	1.101056
-827.601610	-32.736053	1.106061
-831.306798	-30.618948	1.111066
-835.541638	-23.524170	1.116070
-839.383442	-27.501864	1.121075
-842.879682	-37.757081	1.126080
-846.674976	-25.271875	1.131085
-849.958082	-34.965099	1.136090
-854.003312	-17.863872	1.141094
-857.794578	-28.049837	1.146099
-861.816609	-28.646273	1.151104
-865.454843	-36.212284	1.156109
-869.025801	-35.808550	1.161114
-872.442558	-34.771909	1.166118
-876.265249	-30.642798	1.171123
-880.079842	-31.289710	1.176128
-884.321368	-23.775912	1.181133
-887.781680	-40.244903	1.186138
-891.622676	-36.934386	1.191142
-895.495530	-31.502623	1.196147
-898.967157	-32.797233	1.201152
-903.008209	-20.865550	1.206157
-906.552055	-36.764527	1.211162
-910.731434	-35.514450	1.216166
-914.456211	-39.015589	1.221171
-917.789389	-35.978596	1.226176
-921.758583	-40.591754	1.231181
-925.300104	-26.300504	1.236186
-929.009478	-31.767276	1.241190
-933.012875	-29.113506	1.246195
-936.602957	-30.952061	1.251200
-940.852303	-26.983274	1.256205
-944.398337	-30.631211	1.261210
-948.438266	-32.815688	1.266214
-951.953745	-34.908983	1.271219
-955.302896	-22.004546	1.276224
-959.276357	-42.724578	1.281229
-962.740550	-11.182172	1.286234
-966.597292	-43.903418	1.291238
-970.648185	-10.114777	1.296243
-974.066333	-51.520515	1.301248
-978.139525	-37.186763	1.306253
-981.698585	-30.464710	1.311258
-985.400466	-38.663704	1.316262
-989.553944	-47.096383	1.321267
-993.057405	-24.233019	1.326272
-997.131326	-28.572275	1.331277
-1000.789009	-40.920718	1.336282
-1004.540713	-44.639740	1.341286
-1008.137308	-34.723242	1.346291
-1012.067091	-30.160499	1.351296
-1016.179077	-25.822484	1.356301
-1019.494320	-40.993047	1.361306
-1023.374602	-30.512370	1.366310
-1026.830458	-23.546571	1.371315
-1030.527163	-37.561774	1.376320
-1034.863662	-22.149813	1.381325
-1038.693935	-25.832566	1.386330
-1042.447533	-23.740503	1.391334
-1045.898713	-37.673528	1.396339
-1049.161146	-37.903878	1.401344
-1052.866923	-29.865233	1.406349
-1056.819036	-34.391007	1.411354
-1060.961653	-32.548915	1.416358
-1064.587433	-25.874412	1.421363
-1068.449314	-31.415904	1.426368
-1072.459678	-33.369941	1.431373
-1075.824339	-42.004318	1.436378
-1079.852173	-39.040484	1.441382
-1083.572102	-34.962172	1.446387
-1087.125800	-45.212532	1.451392
-1090.848165	-27.375744	1.456397
-1094.637482	-43.038024	1.461402
-1098.457940	-34.466914	1.466406
-1102.591250	-31.243334	1.471411
-1105.894602	-34.169791	1.476416
-1109.885484	-23.655516	1.481421
-1113.681735	-37.667266	1.486426
-1117.112229	-27.619491	1.491430
-1121.267404	-25.622328	1.496435
-1124.727011	-38.077937	1.501440
-1128.561146	-23.208200	1.506445
-1132.092011	-35.687091	1.511450
-1136.265107	-34.981635	1.516454
-1140.112699	-30.819737	1.521459
-1143.414619	-36.840161	1.526464
-1147.489310	-31.356784	1.531469
-1151.004433	-31.589142	1.536474
-1154.936732	-34.653015	1.541478
-1158.850143	-27.216465	1.546483
-1162.450463	-31.692687	1.551488
-1166.786875	-22.860737	1.556493
-1169.912688	-33.097428	1.561498
-1173.808197	-35.042857	1.566502
-1177.256422	-28.465977	1.571507
-1180.906402	-37.169656	1.576512
-1185.008538	-25.949955	1.581517
-1188.740745	-32.565326	1.586522
-1192.554357	-31.212430	1.591526
-1196.468176	-33.527029	1.596531
-1199.671700	-44.069759	1.601536
-1204.135890	-29.382942	1.606541
-1207.730601	-29.422717	1.611546
-1211.467286	-31.866551	1.616550
-1214.958504	-26.662486	1.621555
-1218.296022	-32.880518	1.626560
-1222.669711	-29.061636	1.631565
-1226.159298	-38.010087	1.636570
-1230.121986	-20.602968	1.641574
-1234.094031	-26.519186	1.646579
-1237.558844	-31.179387	1.651584
-1241.737362	-29.048975	1.656589
-1245.223685	-40.911943	1.661594
-1249.077420	-35.705012	1.666598
-1253.092178	-27.037916	1.671603
-1256.114584	-28.974697	1.676608
-1260.020505	-26.843721	1.681613
-1263.576404	-41.906000	1.686618
-1267.680095	-35.131069	1.691622
-1271.683486	-28.189263	1.696627
-1275.541224	-32.685606	1.701632
-1279.264098	-28.647516	1.706637
-1282.655879	-41.170485	1.711642
-1286.179586	-31.101258	1.716646
-1290.299289	-30.528642	1.721651
-1294.006265	-35.321876	1.726656
-1298.180748	-24.267016	1.731661
-1301.903676	-31.265281	1.736666
-1305.526406	-23.438228	1.741670
-1309.189877	-38.776511	1.746675
-1312.430283	-40.042854	1.751680
-1316.587208	-21.842898	1.756685
-1320.321104	-33.251413	1.761690
-1324.028347	-26.554025	1.766694
-1328.116108	-32.375864	1.771699
-1331.702973	-40.064437	1.776704
-1335.840250	-27.571075	1.781709
-1339.302552	-21.996165	1.786714
-1342.908642	-24.356616	1.791718
-1346.696837	-28.813510	1.796723
-1350.266909	-35.616975	1.801728
-1354.176041	-38.688941	1.806733
-1357.942659	-20.653888	1.811738
-1362.091471	-29.435108	1.816742
-1365.614735	-37.255225	1.821747
-1369.326074	-34.437748	1.826752
-1373.129099	-20.050410	1.831757
-1376.991656	-39.156922	1.836762
-1380.907212	-21.493785	1.841766
-1383.917902	-32.798776	1.846771
-1387.839040	-35.490318	1.851776
-1391.967289	-43.541528	1.856781
-1395.407989	-37.952656	1.861786
-1399.140050	-21.805838	1.866790
-1403.111774	-27.251903	1.871795
-1406.808055	-39.465748	1.876800
-1410.869547	-23.862226	1.881805
-1414.851759	-34.696269	1.886810
-1418.370100	-35.544253	1.891814
-1421.862905	-37.296701	1.896819
-1425.490813	-40.568097	1.901824
-1429.242297	-30.028567	1.906829
-1432.926897	-33.257763	1.911834
-1436.790512	-32.128260	1.916838
-1440.978534	-35.727822	1.921843
-1444.723799	-41.178527	1.926848
-1448.741954	-33.513447	1.931853
-1451.950025	-38.157652	1.936858
-1455.881758	-28.787627	1.941862
-1459.846985	-23.092600	1.946867
-1463.447448	-31.053157	1.951872
-1467.025597	-22.908170	1.956877
-1470.777812	-29.972419	1.961882
-1474.376299	-34.372743	1.966886
-1478.271027	-29.021691	1.971891
-1482.043353	-39.067673	1.976896
-1485.938885	-32.128593	1.981901
-1489.497068	-35.042069	1.986906
-1493.734996	-42.802730	1.991910
-1497.370077	-29.558518	1.996915
-1501.182545	-32.888474	2.006912
-1502.006923	-34.309999	2.016909
-1499.525024	-28.328718	2.026906
-1496.770047	-35.143686	2.036902
-1494.579757	-28.146280	2.046899
-1492.803250	-30.716873	2.056896
-1490.671778	-31.681754	2.066893
-1489.073195	-30.642978	2.076890
-1487.339497	-33.835102	2.086886
-1485.313070	-32.219075	2.096883
-1482.886064	-34.887503	2.106880
-1481.131808	-36.292476	2.116877
-1479.447892	-34.356351	2.126874
-1477.703466	-35.372925	2.136870
-1475.677997	-25.988697	2.146867
-1473.678971	-28.735425	2.156864
-1471.882105	-36.180074	2.166861
-1470.177597	-34.874049	2.176858
-1467.862071	-33.430605	2.186854
-1466.068778	-34.118696	2.196851
-1464.249978	-33.314100	2.206848
-1462.466250	-30.364520	2.216845
-1460.543204	-31.888077	2.226842
-1458.481966	-25.233109	2.236838
-1456.677082	-31.122267	2.246835
-1454.895217	-30.044922	2.256832
-1452.877253	-33.022021	2.266829
-1451.255524	-33.494745	2.276826
-1449.286516	-25.400861	2.286822
-1447.664087	-30.506101	2.296819
-1445.088419	-42.185217	2.306816
-1443.514575	-29.498286	2.316813
-1441.597998	-31.709180	2.326810
-1440.081191	-38.270587	2.336806
-1437.837163	-23.651046	2.346803
-1435.908663	-38.932152	2.356800
-1434.227571	-32.991527	2.366797
-1432.451713	-39.333890	2.376794
-1430.562173	-39.213192	2.386790
-1428.299591	-35.424505	2.396787
-1426.709479	-36.121086	2.406784
-1424.915467	-33.340483	2.416781
-1422.872836	-35.266820	2.426778
-1421.091987	-31.906239	2.436774
-1419.175956	-37.622119	2.446771
-1416.972989	-29.497770	2.456768
-1415.223614	-34.236487	2.466765
-1413.636103	-34.381618	2.476762
-1411.552616	-32.283630	2.486758
-1409.670754	-33.413730	2.496755
-1407.896470	-31.973573	2.506752
-1406.110870	-23.326100	2.516749
-1404.277644	-28.446111	2.526746
-1402.110687	-26.140435	2.536742
-1400.252339	-32.761234	2.546739
-1398.496520	-33.531689	2.556736
-1396.525537	-33.225063	2.566733
-1394.261483	-30.717039	2.576730
-1393.072280	-30.001064	2.586726
-1390.794885	-28.158297	2.596723
-1389.114844	-31.847000	2.606720
-1387.070669	-37.643365	2.616717
-1385.070065	-29.657107	2.626714
-1383.366957	-25.620924	2.636710
-1381.684190	-36.934426	2.646707
-1379.934763	-23.970823	2.656704
-1377.783501	-39.794367	2.666701
-1375.873198	-32.164681	2.676698
-1374.102146	-31.169221	2.686694
-1372.079802	-33.913280	2.696691
-1370.311643	-32.099499	2.706688
-1368.290566	-32.828713	2.716685
-1366.145663	-37.496503	2.726682
-1364.874105	-29.811927	2.736678
-1362.779508	-33.565391	2.746675
-1360.662920	-23.156736	2.756672
-1359.145462	-37.710450	2.766669
-1357.349864	-24.894738	2.776666
-1355.296561	-26.697995	2.786662
-1353.504567	-32.660801	2.796659
-1351.539027	-25.448859	2.806656
-1349.517666	-35.872374	2.816653
-1347.512219	-39.163154	2.826650
-1345.841642	-26.403207	2.836646
-1343.881294	-33.032396	2.846643
-1342.253189	-33.690793	2.856640
-1340.259649	-28.491648	2.866637
-1338.148912	-32.958166	2.876634
-1336.522841	-27.987555	2.886630
-1334.587707	-24.166883	2.896627
-1332.834730	-31.378634	2.906624
-1330.747241	-29.622248	2.916621
-1328.912342	-33.147809	2.926618
-1327.107097	-28.196396	2.936614
-1325.305351	-32.501348	2.946611
-1323.316051	-39.926167	2.956608
-1321.504072	-31.672829	2.966605
-1319.397622	-32.807225	2.976602
-1317.538582	-38.591269	2.986598
-1315.837797	-30.836420	2.996595
-1314.065640	-24.125571	3.006592
-1311.952044	-41.978201	3.016589
-1310.340362	-25.632653	3.026586
-1308.319023	-35.004604	3.036582
-1306.354098	-25.768407	3.046579
-1304.592180	-33.753638	3.056576
-1302.661661	-38.000238	3.066573
-1300.699765	-34.987468	3.076570
-1298.964829	-28.737997	3.086566
-1297.170022	-31.642937	3.096563
-1295.139665	-30.017895	3.106560
-1293.129439	-27.044429	3.116557
-1291.327932	-31.453524	3.126554
-1289.480601	-31.027548	3.136550
-1287.574162	-30.069477	3.146547
-1286.097493	-41.095736	3.156544
-1283.961655	-32.300539	3.166541
-1282.038570	-28.446316	3.176538
-1279.860159	-30.503203	3.186534
-1278.309436	-36.768379	3.196531
-1276.562868	-26.977761	3.206528
-1274.612752	-28.611284	3.216525
-1272.648747	-35.422573	3.226522
-1270.717242	-19.717084	3.236518
-1268.693186	-24.925954	3.246515
-1266.861027	-24.123339	3.256512
-1265.192421	-28.624827	3.266509
-1263.229682	-19.902948	3.276506
-1261.282869	-29.602398	3.286502
-1259.614951	-25.645746	3.296499
-1257.623731	-35.598601	3.306496
-1255.676633	-27.339984	3.316493
-1253.896227	-36.687547	3.326490
-1252.062252	-33.436380	3.336486
-1250.210890	-32.142637	3.346483
-1248.189632	-22.866452	3.356480
-1246.237582	-27.972206	3.366477
-1244.522939	-33.638360	3.376474
-1242.320900	-30.324507	3.386470
-1240.797674	-25.866288	3.396467
-1238.869736	-27.129934	3.406464
-1237.072791	-25.868523	3.416461
-1235.201710	-34.635350	3.426458
-1233.257361	-28.979835	3.436454
-1231.334074	-30.323253	3.446451
-1229.666678	-29.833702	3.456448
-1227.629249	-34.809423	3.466445
-1225.672402	-30.867400	3.476442
-1223.754448	-30.039007	3.486438
-1221.817564	-28.629458	3.496435
-1220.356038	-20.398892	3.506432
-1218.160658	-34.350520	3.516429
-1216.076505	-34.346044	3.526426
-1214.309112	-26.770707	3.536422
-1212.603400	-30.412873	3.546419
-1211.021471	-26.677677	3.556416
-1209.063724	-32.223239	3.566413
-1206.627029	-31.593089	3.576410
-1205.042231	-30.870841	3.586406
-1203.054370	-25.888545	3.596403
-1201.413562	-24.720539	3.606400
-1199.441757	-26.982705	3.616397
-1197.673571	-25.119847	3.626394
-1195.678669	-23.320103	3.636390
-1193.742526	-20.121544	3.646387
-1191.875352	-28.071440	3.656384
-1190.048461	-32.179799	3.666381
-1188.369590	-26.314407	3.676378
-1186.298838	-34.476859	3.686374
-1184.342096	-37.909704	3.696371
-1182.601744	-23.995568	3.706368
-1180.660218	-37.170793	3.716365
-1178.793020	-35.115351	3.726362
-1176.785649	-32.261319	3.736358
-1175.275427	-34.891701	3.746355
-1172.970324	-29.971186	3.756352
-1171.369974	-35.109027	3.766349
-1169.381786	-37.111695	3.776346
-1167.398978	-43.095420	3.786342
-1165.966864	-31.961305	3.796339
-1163.617586	-31.588691	3.806336
-1161.781351	-33.391788	3.816333
-1160.395602	-27.430535	3.826330
-1158.197613	-32.771344	3.836326
-1156.259979	-19.984481	3.846323
-1154.404285	-25.524728	3.856320
-1152.639201	-33.826139	3.866317
-1150.553605	-29.470456	3.876314
-1148.795871	-26.552778	3.886310
-1147.007927	-26.732949	3.896307
-1145.095461	-31.585985	3.906304
-1143.061893	-26.178334	3.916301
-1141.077667	-31.238627	3.926298
-1139.242288	-30.022760	3.936294
-1137.615267	-29.837722	3.946291
-1135.836026	-27.553446	3.956288
-1133.803168	-29.367451	3.966285
-1131.817606	-33.793242	3.976282
-1129.827324	-28.264976	3.986278
-1128.394414	-37.171622	3.996275
-1126.354800	-27.107241	4.006272
-1124.146601	-26.295196	4.016269
-1122.775685	-27.684369	4.026266
-1120.448329	-33.072681	4.036262
-1118.704048	-38.370874	4.046259
-1116.902896	-38.411036	4.056256
-1115.019009	-28.509621	4.066253
-1113.249463	-28.105796	4.076250
-1111.170358	-34.848535	4.086246
-1109.468316	-25.915874	4.096243
-1107.640488	-32.050021	4.106240
-1105.290503	-26.206655	4.116237
-1103.818264	-30.907140	4.126234
-1101.935188	-35.319671	4.136230
-1099.778126	-29.492807	4.146227
-1098.214485	-25.118317	4.156224
-1096.219351	-31.001336	4.166221
-1094.253438	-38.875375	4.176218
-1092.423524	-36.864423	4.186214
-1090.502442	-34.004406	4.196211
-1088.850987	-28.437695	4.206208
-1086.755468	-35.058309	4.216205
-1085.001032	-31.873224	4.226202
-1083.087021	-35.190212	4.236198
-1081.425080	-30.735123	4.246195
-1079.433535	-38.087486	4.256192
-1077.458500	-39.879562	4.266189
-1075.376747	-35.104793	4.276186
-1073.702862	-37.620769	4.286182
-1072.013078	-33.716418	4.296179
-1070.052485	-25.639778	4.306176
-1067.839868	-34.885830	4.316173
-1066.037061	-35.101473	4.326170
-1064.542410	-37.708770	4.336166
-1062.043619	-30.569219	4.346163
-1060.721177	-28.186561	4.356160
-1058.799072	-34.670473	4.366157
-1056.932634	-32.351137	4.376154
-1055.083330	-30.850074	4.386150
-1053.040568	-32.266138	4.396147
-1051.060915	-45.300529	4.406144
-1049.372434	-36.518806	4.416141
-1047.394697	-42.904240	4.426138
-1045.612841	-32.875924	4.436134
-1043.888605	-33.045827	4.446131
-1041.696204	-31.689622	4.456128
-1039.742401	-39.425900	4.466125
-1038.017722	-27.950073	4.476122
-1035.968386	-37.686277	4.486118
-1034.525126	-28.945842	4.496115
-1032.632023	-32.336812	4.506112
-1030.623484	-31.338016	4.516109
-1028.719373	-26.931089	4.526106
-1026.760444	-29.933127	4.536102
-1024.629332	-23.058398	4.546099
-1022.775483	-31.377077	4.556096
-1021.297389	-27.625139	4.566093
-1019.463181	-34.158120	4.576090
-1017.586452	-25.809083	4.586086
-1015.492790	-36.346537	4.596083
-1013.611633	-38.273540	4.606080
-1011.707338	-38.630102	4.616077
-1009.894582	-35.620068	4.626074
-1008.300059	-34.862926	4.636070
-1006.253637	-32.131823	4.646067
-1004.326228	-29.530101	4.656064
-1002.335198	-34.245597	4.666061
-1000.655900	-30.066368	4.676058
-998.540562	-40.086242	4.686054
-996.699207	-36.209231	4.696051
-995.136046	-31.589866	4.706048
-992.950713	-29.206213	4.716045
-991.002236	-35.040636	4.726042
-988.962043	-33.420052	4.736038
-987.615621	-25.946145	4.746035
-985.553847	-31.323439	4.756032
-983.497169	-26.489310	4.766029
-981.930147	-25.029887	4.776026
-979.918588	-37.133062	4.786022
-978.115169	-29.037521	4.796019
-976.235691	-31.232637	4.806016
-974.176566	-24.993688	4.816013
-972.231146	-26.975145	4.826010
-970.592780	-26.041837	4.836006
-968.967779	-36.546944	4.846003
-966.759332	-22.132749	4.856000
-964.664083	-30.131582	4.865997
-962.897530	-31.726025	4.875994
-961.297782	-36.759433	4.885990
-959.206534	-31.237683	4.895987
-957.277738	-22.320625	4.905984
-955.783188	-21.586932	4.915981
-953.592709	-23.520720	4.925978
-951.613173	-26.683880	4.935974
-949.934516	-26.601700	4.945971
-948.032386	-31.973963	4.955968
-946.218289	-28.378326	4.965965
-944.141682	-25.915666	4.975962
-942.636104	-27.012070	4.985958
-940.373635	-30.291509	4.995955
-938.341725	-23.413465	5.005952
-936.666242	-24.355460	5.015949
-935.070761	-34.620576	5.025946
-932.830459	-28.514764	5.035942
-931.183298	-29.145925	5.045939
-929.277819	-28.177930	5.055936
-927.628134	-28.901067	5.065933
-925.477127	-27.643917	5.075930
-923.418905	-32.197996	5.085926
-921.658263	-32.499940	5.095923
-919.898744	-32.285410	5.105920
-918.244087	-31.812545	5.115917
-915.981123	-26.633982	5.125914
-914.234090	-36.672273	5.135910
-912.236164	-41.128283	5.145907
-910.503554	-40.221053	5.155904
-908.597989	-25.482069	5.165901
-906.648908	-29.030307	5.175898
-904.985350	-32.015023	5.185894
-903.012123	-25.680173	5.195891
-901.096337	-22.593366	5.205888
-899.127501	-32.705003	5.215885
-897.321746	-22.723001	5.225882
-895.543121	-20.422647	5.235878
-893.362293	-25.675223	5.245875
-891.851294	-27.959781	5.255872
-889.984725	-20.846844	5.265869
-887.759069	-23.070395	5.275866
-886.121040	-26.060491	5.285862
-884.082465	-25.508456	5.295859
-882.260196	-26.789655	5.305856
-880.530576	-23.166249	5.315853
-878.674616	-31.467798	5.325850
-876.730303	-34.415274	5.335846
-875.073877	-29.657581	5.345843
-872.856173	-27.978432	5.355840
-870.871935	-22.911573	5.365837
-869.446062	-31.333828	5.375834
-867.563633	-29.432137	5.385830
-865.335183	-21.857577	5.395827
-863.169859	-21.141056	5.405824
-861.734254	-22.199384	5.415821
-859.844355	-24.115036	5.425818
-857.780899	-23.983780	5.435814
-856.018987	-21.156535	5.445811
-854.319472	-26.322665	5.455808
-852.605388	-27.884956	5.465805
-850.522089	-30.775686	5.475802
-848.510392	-25.260059	5.485798
-846.500097	-26.119727	5.495795
-844.718999	-28.919516	5.505792
-842.820579	-28.706605	5.515789
-841.228962	-32.543426	5.525786
-839.301729	-23.392336	5.535782
-837.108529	-26.376409	5.545779
-835.303089	-21.891965	5.555776
-833.397628	-23.582724	5.565773
-831.920466	-24.805565	5.575770
-829.582522	-31.949435	5.585766
-827.913067	-33.779301	5.595763
-826.373925	-31.104314	5.605760
-824.178624	-27.160579	5.615757
-822.329892	-31.805822	5.625754
-820.187103	-23.919117	5.635750
-818.287337	-26.406289	5.645747
-816.742143	-25.396404	5.655744
-815.108917	-27.040478	5.665741
-812.922141	-29.426684	5.675738
-810.694619	-23.864995	5.685734
-808.953217	-34.161258	5.695731
-807.396168	-31.394388	5.705728
-805.375296	-26.521214	5.715725
-803.518347	-26.097967	5.725722
-801.783726	-28.413474	5.735718
-800.044452	-29.190314	5.745715
-797.644006	-26.304035	5.755712
-795.764991	-32.266149	5.765709
-794.374934	-29.118910	5.775706
-792.409422	-26.791507	5.785702
-789.992219	-27.083030	5.795699
-788.742576	-28.558416	5.805696
-786.732700	-29.784267	5.815693
-784.560378	-25.410523	5.825690
-782.906745	-32.909173	5.835686
-780.951550	-26.896580	5.845683
-779.195161	-16.518175	5.855680
-777.060125	-23.874299	5.865677
-775.490263	-28.928079	5.875674
-773.636743	-27.531669	5.885670
-771.602814	-30.626012	5.895667
-769.723706	-26.366438	5.905664
-767.980347	-25.334508	5.915661
-766.086370	-31.303729	5.925658
-763.954229	-24.165235	5.935654
-762.205316	-26.539838	5.945651
-760.421114	-29.799517	5.955648
-758.691232	-24.039830	5.965645
-756.684061	-25.331537	5.975642
-754.664683	-26.740452	5.985638
-752.565076	-25.009157	5.995635
-750.823631	-30.494536	6.005632
-749.215391	-22.323395	6.015629
-747.415453	-21.039975	6.025626
-745.347993	-25.413814	6.035622
-743.476635	-29.598424	6.045619
-741.579394	-25.292779	6.055616
-739.965647	-22.842803	6.065613
-737.719791	-24.775771	6.075610
-735.755327	-21.968170	6.085606
-734.170382	-29.545812	6.095603
-732.349682	-12.948947	6.105600
-730.235142	-30.837648	6.115597
-728.304828	-28.671927	6.125594
-726.581406	-33.237077	6.135590
-724.542302	-30.802960	6.145587
-723.111509	-22.183460	6.155584
-721.324856	-28.324965	6.165581
-719.038271	-12.012524	6.175578
-716.917284	-27.110781	6.185574
-715.371596	-24.970426	6.195571
-713.366307	-27.261230	6.205568
-711.400732	-21.897573	6.215565
-709.770225	-24.698464	6.225562
-707.909512	-25.406224	6.235558
-705.855524	-30.398378	6.245555
-704.054493	-26.170482	6.255552
-702.384973	-20.697934	6.265549
-700.237048	-37.068318	6.275546
-698.342826	-28.429700	6.285542
-696.506774	-28.197232	6.295539
-695.098093	-30.830042	6.305536
-692.846547	-26.732541	6.315533
-690.903982	-27.593887	6.325530
-689.050535	-25.431639	6.335526
-687.157350	-19.859033	6.345523
-685.263303	-27.774972	6.355520
-683.562678	-32.374344	6.365517
-681.595832	-30.681771	6.375514
-679.545107	-30.085712	6.385510
-677.648315	-32.207577	6.395507
-675.815633	-22.747557	6.405504
-673.990115	-24.401735	6.415501
-672.473179	-23.150405	6.425498
-670.235951	-28.544425	6.435494
-668.245774	-27.648167	6.445491
-666.614986	-22.698331	6.455488
-664.684041	-29.803866	6.465485
-662.902689	-27.892173	6.475482
-661.069055	-23.219469	6.485478
-658.980603	-20.580026	6.495475
-657.004002	-28.199673	6.505472
-655.330256	-22.075685	6.515469
-653.334350	-23.390769	6.525466
-651.548623	-27.866355	6.535462
-649.600560	-31.207394	6.545459
-647.856168	-32.907009	6.555456
-645.833164	-28.622955	6.565453
-644.037431	-27.307206	6.575450
-642.415145	-32.242969	6.585446
-640.242697	-18.190539	6.595443
-638.374095	-26.861824	6.605440
-636.485744	-25.049307	6.615437
-634.756112	-28.576483	6.625434
-632.704364	-24.715412	6.635430
-630.637581	-31.353169	6.645427
-629.071898	-24.888227	6.655424
-627.221923	-24.661087	6.665421
-625.568775	-27.102396	6.675418
-623.298590	-24.910360	6.685414
-621.248096	-24.985239	6.695411
-619.457191	-21.944556	6.705408
-617.826738	-30.217794	6.715405
-616.191703	-33.169340	6.725402
-613.940591	-28.740126	6.735398
-611.899956	-25.883011	6.745395
-610.368243	-34.887281	6.755392
-608.500416	-25.818066	6.765389
-606.548456	-34.066869	6.775386
-604.614027	-32.837981	6.785382
-602.796154	-28.704269	6.795379
-600.989565	-29.456982	6.805376
-598.904814	-35.622337	6.815373
-596.928161	-33.343914	6.825370
-595.270357	-31.232441	6.835366
-593.368942	-33.561813	6.845363
-591.479295	-30.254264	6.855360
-589.750497	-27.920452	6.865357
-587.783581	-26.581480	6.875354
-585.666495	-33.688269	6.885350
-584.143668	-28.754285	6.895347
-582.269869	-30.596098	6.905344
-580.159274	-33.847786	6.915341
-578.395772	-25.125023	6.925338
-576.500502	-27.551292	6.935334
-574.609786	-30.379448	6.945331
-572.626267	-28.143151	6.955328
-570.796654	-25.195453	6.965325
-569.001255	-27.888384	6.975322
-567.018154	-23.662618	6.985318
-565.111561	-28.302707	6.995315
-563.447145	-25.791229	7.005312
-561.754722	-24.068930	7.015309
-559.623953	-19.432549	7.025306
-557.655689	-30.446975	7.035302
-555.545889	-34.326912	7.045299
-554.121269	-28.148846	7.055296
-552.122143	-30.716417	7.065293
-550.501558	-27.634267	7.075290
-548.140656	-29.891738	7.085286
-546.506040	-25.959228	7.095283
-544.859850	-22.393286	7.105280
-542.351064	-25.776436	7.115277
-540.791424	-32.989936	7.125274
-538.988040	-26.332377	7.135270
-537.209035	-25.542801	7.145267
-535.130640	-30.295566	7.155264
-533.284072	-24.064883	7.165261
-531.502627	-31.749577	7.175258
-529.838498	-31.811614	7.185254
-527.681556	-37.865288	7.195251
-525.641883	-20.441135	7.205248
-524.093499	-32.329492	7.215245
-522.101844	-22.864728	7.225242
-520.208647	-25.784815	7.235238
-518.108659	-28.553197	7.245235
-516.618655	-31.430991	7.255232
-514.629206	-31.916013	7.265229
-512.418596	-22.172010	7.275226
-510.959303	-35.964477	7.285222
-509.049937	-25.174505	7.295219
-507.107143	-31.931303	7.305216
-505.392853	-26.699432	7.315213
-503.179821	-30.178987	7.325210
-501.397845	-30.687703	7.335206
-499.306802	-29.231118	7.345203
-497.723688	-29.584920	7.355200
-495.712673	-25.564068	7.365197
-493.913969	-27.995378	7.375194
-492.008634	-27.855919	7.385190
-490.184640	-34.236903	7.395187
-488.223176	-33.334329	7.405184
-486.194374	-27.870050	7.415181
-484.593854	-29.857613	7.425178
-483.036163	-36.728148	7.435174
-480.795057	-30.721476	7.445171
-478.931404	-28.368065	7.455168
-477.026663	-29.439506	7.465165
-475.371348	-28.544871	7.475162
-473.218080	-30.093349	7.485158
-471.324269	-26.724786	7.495155
-469.450843	-36.519309	7.505152
-467.549702	-30.699904	7.515149
-465.798421	-30.493193	7.525146
-463.778667	-29.153082	7.535142
-461.892285	-29.015309	7.545139
-460.094314	-23.492039	7.555136
-458.176707	-22.809796	7.565133
-456.691754	-29.229773	7.575130
-454.538982	-28.326142	7.585126
-452.680024	-31.753848	7.595123
-450.488692	-26.699159	7.605120
-448.953891	-22.761690	7.615117
-447.047632	-27.908460	7.625114
-444.952420	-26.525120	7.635110
-443.207213	-26.448471	7.645107
-441.647875	-26.479504	7.655104
-439.480846	-23.517686	7.665101
-437.572205	-23.486075	7.675098
-435.658295	-20.368577	7.685094
-433.867953	-24.780014	7.695091
-431.751804	-30.288696	7.705088
-430.376984	-27.424576	7.715085
-428.556360	-23.696936	7.725082
-426.425802	-28.852665	7.735078
-424.340674	-21.482129	7.745075
-422.483497	-30.124598	7.755072
-420.880249	-30.140525	7.765069
-419.003459	-25.540826	7.775066
-417.085226	-24.877596	7.785062
-414.942657	-24.662274	7.795059
-413.088794	-28.079665	7.805056
-411.369973	-21.676907	7.815053
-409.504427	-25.561933	7.825050
-407.437703	-20.523619	7.835046
-405.754320	-17.906110	7.845043
-403.960322	-28.452095	7.855040
-401.974407	-18.481054	7.865037
-400.192993	-19.684318	7.875034
-398.241267	-22.774705	7.885030
-396.219620	-22.691633	7.895027
-394.612566	-15.723140	7.905024
-392.881707	-14.928925	7.915021
-390.575770	-23.873543	7.925018
-388.891362	-20.023073	7.935014
-386.792091	-27.027391	7.945011
-385.006204	-24.884112	7.955008
-383.319597	-16.902033	7.965005
-381.224335	-23.822027	7.975002
-379.507850	-23.038139	7.984998
-377.770196	-23.653369	7.994995
-375.742249	-30.177359	8.004992
-373.791905	-28.159797	8.014989
-371.941555	-19.228099	8.024986
-370.024192	-21.084601	8.034982
-368.463400	-21.973156	8.044979
-366.085957	-22.150538	8.054976
-364.346090	-20.939335	8.064973
-362.543616	-20.164426	8.074970
-360.696291	-24.790165	8.084966
-358.893735	-26.514649	8.094963
-356.894301	-23.710728	8.104960
-355.259411	-18.942887	8.114957
-353.222591	-23.663607	8.124954
-351.237073	-20.483262	8.134950
-349.518839	-16.840260	8.144947
-347.899039	-23.392229	8.154944
-345.716553	-25.516818	8.164941
-343.833121	-30.541451	8.174938
-341.808581	-18.835004	8.184934
-339.852812	-21.805995	8.194931
-337.853381	-19.777292	8.204928
-336.561605	-18.300333	8.214925
-334.434459	-29.467856	8.224922
-332.504467	-21.414071	8.234918
-330.547314	-12.780424	8.244915
-328.990754	-12.662525	8.254912
-326.979838	-20.421614	8.264909
-325.175819	-18.743797	8.274906
-323.365426	-23.005206	8.284902
-321.398712	-18.839763	8.294899
-319.306020	-14.211286	8.304896
-317.380431	-12.631813	8.314893
-315.580064	-15.025367	8.324890
-313.803239	-17.274641	8.334886
-311.980610	-21.440104	8.344883
-310.043040	-17.000009	8.354880
-308.224959	-21.553151	8.364877
-306.297727	-17.305605	8.374874
-304.298409	-27.805357	8.384870
-302.516420	-35.191575	8.394867
-301.025958	-20.261006	8.404864
-298.628542	-27.964926	8.414861
-296.748219	-30.919102	8.424858
-295.239739	-14.977751	8.434854
-293.085765	-24.063813	8.444851
-291.071392	-20.270675	8.454848
-289.388222	-21.156609	8.464845
-287.631097	-22.447489	8.474842
-285.604074	-25.426653	8.484838
-283.733034	-25.066824	8.494835
-282.011029	-20.867026	8.504832
-280.232030	-17.123148	8.514829
-278.230699	-26.385352	8.524826
-276.195498	-28.039544	8.534822
-274.427154	-19.070989	8.544819
-272.341124	-20.366988	8.554816
-270.589966	-26.987242	8.564813
-269.225558	-19.228376	8.574810
-266.877898	-27.936395	8.584807
-264.874337	-29.223962	8.594803
-262.908806	-34.181115	8.604800
-261.220545	-23.821398	8.614797
-259.360845	-24.148138	8.624794
-257.567941	-18.917567	8.634791
-255.419084	-22.981904	8.644787
-253.850051	-29.348876	8.654784
-251.988279	-22.837760	8.664781
-249.925794	-22.265310	8.674778
-248.304435	-24.383938	8.684775
-246.238311	-21.873187	8.694771
-244.273247	-31.829024	8.704768
-242.212484	-29.686876	8.714765
-240.610413	-28.202547	8.724762
-238.847978	-31.627322	8.734759
-236.835181	-32.753713	8.744755
-234.916784	-29.455193	8.754752
-233.012464	-28.099619	8.764749
-231.273173	-24.523046	8.774746
-229.661623	-20.016643	8.784743
-227.473168	-26.930860	8.794739
-225.273880	-21.978270	8.804736
-223.593378	-29.795069	8.814733
-222.127752	-35.976576	8.824730
-219.952043	-27.068254	8.834727
-218.127847	-27.924540	8.844723
-216.234337	-31.905462	8.854720
-214.474347	-37.259234	8.864717
-212.608891	-33.015966	8.874714
-210.758059	-27.437775	8.884711
-208.572549	-30.634792	8.894707
-206.755637	-32.484610	8.904704
-204.925636	-23.445315	8.914701
-203.118642	-22.464172	8.924698
-201.335524	-19.635069	8.934695
-199.556747	-33.509958	8.944691
-197.189119	-31.287270	8.954688
-195.580123	-35.767491	8.964685
-193.781290	-27.133728	8.974682
-191.749157	-28.264747	8.984679
-189.907254	-28.345444	8.994675
-188.217118	-32.881239	9.004672
-186.602220	-31.406815	9.014669
-184.561622	-28.009336	9.024666
-182.430171	-28.418853	9.034663
-180.302910	-23.653666	9.044659
-178.689957	-27.675053	9.054656
-176.733661	-31.391237	9.064653
-175.029569	-28.579505	9.074650
-173.099266	-23.519208	9.084647
-171.229208	-24.117524	9.094643
-169.436908	-24.714483	9.104640
-167.414890	-23.447108	9.114637
-165.382319	-33.209983	9.124634
-163.509000	-28.759514	9.134631
-161.950992	-29.017514	9.144627
-160.348238	-27.062729	9.154624
-157.964474	-26.104111	9.164621
-156.194807	-22.824423	9.174618
-154.474284	-29.764964	9.184615
-152.455327	-33.330080	9.194611
-150.293662	-33.289668	9.204608
-148.770010	-31.593824	9.214605
-146.630091	-30.436820	9.224602
-145.164394	-23.132969	9.234599
-142.815612	-19.093068	9.244595
-141.136250	-32.164194	9.254592
-139.314708	-22.408254	9.264589
-137.385405	-21.167111	9.274586
-135.645954	-18.343622	9.284583
-133.788944	-16.775163	9.294579
-131.831399	-18.904725	9.304576
-129.928939	-16.119870	9.314573
-128.165978	-20.521991	9.324570
-126.208553	-23.568867	9.334567
-124.197592	-15.581493	9.344563
-122.419151	-21.214460	9.354560
-120.617257	-14.448947	9.364557
-118.547377	-21.914140	9.374554
-116.680882	-18.381457	9.384551
-114.992002	-23.258048	9.394547
-112.964230	-20.827899	9.404544
-111.260095	-20.496569	9.414541
-109.339815	-19.691318	9.424538
-107.428437	-25.007599	9.434535
-105.575379	-24.210567	9.444531
-103.760174	-21.291775	9.454528
-101.950964	-27.676452	9.464525
-99.743368	-25.942854	9.474522
-97.821504	-27.281985	9.484519
-96.174497	-28.533056	9.494515
-94.232500	-22.216179	9.504512
-92.574336	-26.791023	9.514509
-90.430767	-22.393078	9.524506
-88.598390	-21.832726	9.534503
-86.872118	-25.077950	9.544499
-84.819207	-20.761850	9.554496
-82.857546	-26.784006	9.564493
-81.193882	-19.817996	9.574490
-79.273361	-18.706454	9.584487
-77.598031	-25.660264	9.594483
-75.501083	-19.049151	9.604480
-73.684022	-19.534731	9.614477
-71.781220	-17.209342	9.624474
-70.016797	-18.949639	9.634471
-67.929124	-14.070664	9.644467
-66.082382	-26.195855	9.654464
-64.261864	-23.119991	9.664461
-62.363705	-14.779840	9.674458
-60.456702	-21.025360	9.684455
-58.719633	-27.777435	9.694451
-56.963847	-28.450589	9.704448
-54.678763	-23.783091	9.714445
-53.077602	-29.698771	9.724442
-51.535524	-22.247571	9.734439
-49.168659	-28.296445	9.744435
-47.301164	-22.313421	9.754432
-45.373817	-23.414973	9.764429
-43.303521	-21.102070	9.774426
-41.785963	-16.875791	9.784423
-39.841599	-19.060019	9.794419
-38.142728	-24.050256	9.804416
-36.207212	-16.432860	9.814413
-34.094012	-21.144987	9.824410
-32.480867	-22.715867	9.834407
-30.331581	-15.648863	9.844403
-28.580083	-23.994750	9.854400
-26.539558	-20.413967	9.864397
-24.984090	-20.483585	9.874394
-23.176531	-21.485490	9.884391
-21.268785	-16.929868	9.894387
-19.178143	-20.282112	9.904384
-17.441822	-23.841513	9.914381
-15.382180	-25.609912	9.924378
-13.641248	-18.872484	9.934375
-11.800342	-18.537637	9.944371
-9.809817	-19.925546	9.954368
-7.914305	-26.036566	9.964365
-6.035902	-17.247967	9.974362
-4.831473	-3.793584	9.984359
-3.370915	23.556919	9.994355
-2.060646	72.131414	10.004352
-1.000208	139.094471	10.014349
0.000000	200.875766	10.019354
0.953138	246.252164	10.024359
1.061173	291.621573	10.029363
1.466534	327.237783	10.034368
2.121198	359.569017	10.039373
2.312754	386.431306	10.044378
3.142272	412.884392	10.049383
2.907697	438.401819	10.054387
3.228887	439.501785	10.059392
3.596100	469.087950	10.064397
3.515507	479.830284	10.069402
3.906192	482.447217	10.074407
3.982505	499.767158	10.079411
3.932026	525.040911	10.084416
4.411025	521.533136	10.089421
4.006028	531.483588	10.094426
4.246020	523.021348	10.099431
4.086759	527.730290	10.104435
4.480115	534.897849	10.109440
4.166361	530.598733	10.114445
4.215470	546.167937	10.119450
4.674262	554.862585	10.124455
4.523582	572.351280	10.129459
4.894117	582.178073	10.134464
5.099535	572.082875	10.139469
4.784860	577.772248	10.144474
5.035366	580.392634	10.149479
5.113304	587.884915	10.154483
5.383535	590.084266	10.159488
5.421787	577.905775	10.164493
5.000701	579.079987	10.169498
5.195233	565.837375	10.174503
5.040047	560.686642	10.179507
5.039265	575.729252	10.184512
5.505674	587.620745	10.189517
5.235920	593.998392	10.194522
5.251567	591.515400	10.199527
5.088894	596.481950	10.204531
5.345785	604.161739	10.209536
5.311290	591.710989	10.214541
5.278710	599.684524	10.219546
5.607379	604.194244	10.224551
5.325715	606.517892	10.229555
5.364862	611.400219	10.234560
5.518792	606.882985	10.239565
5.205528	611.659094	10.244570
5.658588	621.679332	10.249575
5.783941	648.183659	10.254579
5.738918	643.089443	10.259584
5.703843	651.161176	10.264589
5.472712	653.038379	10.269594
5.963748	648.491020	10.274599
5.757286	663.326829	10.279603
5.590175	655.372567	10.284608
6.009223	655.540734	10.289613
5.991852	649.063851	10.294618
6.285782	668.151739	10.299623
6.010243	675.925947	10.304627
6.265407	673.947211	10.309632
6.540368	683.716778	10.314637
6.029425	693.348346	10.319642
6.531337	682.146069	10.324647
6.258139	688.828658	10.329651
6.073491	697.622864	10.334656
6.461503	690.797453	10.339661
6.325436	694.736350	10.344666
6.697718	692.101842	10.349671
6.762737	697.071535	10.354675
6.544997	695.844735	10.359680
6.676135	693.940972	10.364685
6.508141	709.421975	10.369690
6.806920	710.115529	10.374695
6.865564	724.743537	10.379699
6.938713	727.217194	10.384704
6.977049	740.695701	10.389709
7.216216	742.086319	10.394714
7.346047	739.709670	10.399719
7.253257	739.462731	10.404723
7.270866	720.501754	10.409728
7.025443	728.069335	10.414733
6.982766	741.519763	10.419738
7.386340	734.445844	10.424743
7.369441	744.443352	10.429747
7.264531	742.916276	10.434752
7.320401	745.788510	10.439757
7.176648	750.321585	10.444762
7.378252	747.239624	10.449767
7.655484	758.483338	10.454771
7.407387	750.456784	10.459776
7.467828	746.402275	10.464781
7.503090	752.259831	10.469786
7.711342	744.016993	10.474791
7.740144	753.524667	10.479795
7.611258	755.175840	10.484800
7.638028	767.760501	10.489805
7.669612	789.012985	10.494810
7.937864	785.625493	10.499815
7.753035	795.917904	10.504819
8.054583	785.053437	10.509824
8.000886	795.556747	10.514829
7.948890	803.483028	10.519834
8.435484	788.490507	10.524839
8.254258	800.688898	10.529843
8.283436	799.804334	10.534848
8.305127	795.532063	10.539853
8.331714	797.344525	10.544858
8.458000	791.746691	10.549863
8.320848	791.188279	10.554867
8.565293	791.952005	10.559872
8.730059	802.944029	10.564877
8.384370	813.866087	10.569882
8.455203	797.750834	10.574887
8.649150	801.362732	10.579891
8.372861	804.125526	10.584896
8.967600	800.849964	10.589901
8.305266	809.029713	10.594906
8.821980	820.840835	10.599911
8.786166	833.713082	10.604915
9.042801	843.020473	10.609920
9.413722	842.459874	10.614925
9.309370	842.539633	10.619930
9.268621	815.007540	10.624935
9.310543	816.913754	10.629939
9.069025	811.191646	10.634944
9.036951	807.348997	10.639949
8.884370	825.254618	10.644954
9.591989	827.750104	10.649959
9.425535	822.476494	10.654963
9.117963	824.753844	10.659968
9.647263	835.916414	10.664973
9.551928	843.207803	10.669978
9.537003	829.340761	10.674983
9.478338	841.231053	10.679987
9.456952	840.838681	10.684992
9.806746	844.051991	10.689997
9.537495	857.019838	10.695002
9.596422	855.261614	10.700007
9.433058	864.949823	10.705011
9.715855	865.313193	10.710016
9.924765	853.621345	10.715021
9.676638	860.367824	10.720026
9.817899	843.131098	10.725031
9.738693	857.905807	10.730035
9.697391	868.044489	10.735040
9.935147	855.619477	10.740045
9.867956	864.466013	10.745050
10.184614	865.093645	10.750055
9.991652	868.059207	10.755059
10.416471	868.100300	10.760064
10.528116	887.143433	10.765069
10.387951	893.601468	10.770074
10.393691	869.297815	10.775079
10.482173	875.553792	10.780083
10.377352	866.521866	10.785088
10.638438	889.961428	10.790093
10.686408	882.704454	10.795098
10.778596	874.751292	10.800103
10.380990	868.560462	10.805107
10.569235	874.677524	10.810112
10.776635	887.376985	10.815117
10.490209	899.354114	10.820122
10.670982	891.008341	10.825127
10.481173	899.018157	10.830131
10.537392	892.769128	10.835136
10.357120	880.189990	10.840141
10.365297	898.847512	10.845146
10.927832	912.457041	10.850151
10.843824	919.773470	10.855155
10.837884	924.215231	10.860160
11.031088	924.047256	10.865165
11.222329	923.169954	10.870170
11.480337	911.987478	10.875175
10.977641	921.370295	10.880179
11.047137	920.788381	10.885184
11.334709	927.427373	10.890189
11.172565	931.580230	10.895194
11.133708	920.825149	10.900199
11.469136	929.850365	10.905203
11.424386	962.400158	10.910208
11.678907	936.856628	10.915213
11.299731	961.672624	10.920218
11.579487	961.738431	10.925223
11.563656	970.116360	10.930227
11.892589	957.061696	10.935232
11.835077	964.749243	10.940237
11.641618	970.919339	10.945242
12.330458	967.513613	10.950247
12.193837	964.916068	10.955251
11.993913	969.831914	10.960256
12.104515	957.307245	10.965261
12.332067	962.804628	10.970266
12.136776	955.789846	10.975271
12.005347	968.653808	10.980275
12.102784	955.203973	10.985280
11.885743	966.409985	10.990285
11.990755	967.266923	10.995290
12.024326	957.271408	11.000295
12.063205	962.562335	11.005299
12.418969	991.120046	11.010304
12.805994	996.867980	11.015309
12.692533	982.507140	11.020314
12.826148	976.860756	11.025319
12.812944	973.891857	11.030323
12.760094	970.831510	11.035328
13.013088	964.793921	11.040333
12.561094	973.470080	11.045338
12.544959	966.347870	11.050343
12.808595	961.376205	11.055347
12.643910	963.236541	11.060352
12.584610	984.682006	11.065357
12.766328	998.237234	11.070362
12.911235	992.671046	11.075367
12.920649	1006.999678	11.080371
13.113538	1003.630465	11.085376
13.185213	1002.202934	11.090381
13.119560	1001.350830	11.095386
13.411420	1011.322932	11.100391
13.609364	999.068154	11.105395
13.220049	996.263319	11.110400
13.440043	1008.304851	11.115405
13.283783	988.805114	11.120410
13.465273	1008.846539	11.125415
13.620219	1011.398666	11.130419
13.650595	990.284285	11.135424
13.775200	995.834371	11.140429
13.502574	1000.399116	11.145434
13.612350	1000.178213	11.150439
13.770677	1006.203906	11.155443
13.599956	1001.246308	11.160448
13.511059	1008.601409	11.165453
13.110781	1010.130310	11.170458
13.827454	997.715529	11.175463
13.737232	1011.987516	11.180467
14.151825	1016.489970	11.185472
14.585052	1019.773594	11.190477
14.149858	1014.038138	11.195482
14.154706	998.452016	11.200487
13.805814	1006.838931	11.205491
13.997917	1009.572793	11.210496
14.472897	1023.262625	11.215501
14.483976	1030.157080	11.220506
14.530936	1002.333092	11.225511
13.922530	1012.250078	11.230515
14.141409	1027.210812	11.235520
14.379124	1028.366719	11.240525
14.551783	1036.006555	11.245530
14.759717	1029.488836	11.250535
14.531610	1040.266151	11.255539
14.833470	1031.407386	11.260544
14.752254	1032.033826	11.265549
14.637987	1029.942073	11.270554
15.130814	1032.555434	11.275559
15.052818	1028.302147	11.280563
14.877322	1034.261242	11.285568
15.008671	1022.229961	11.290573
14.799030	1032.039205	11.295578
15.207712	1025.858487	11.300583
14.850396	1032.270790	11.305587
14.997925	1037.468720	11.310592
14.982205	1035.856424	11.315597
14.999108	1036.383635	11.320602
15.127377	1030.246061	11.325607
15.048043	1040.297886	11.330611
14.745925	1039.202788	11.335616
15.317623	1040.187154	11.340621
15.292737	1040.183275	11.345626
15.147819	1031.734821	11.350631
15.280653	1042.009858	11.355635
15.312314	1042.276089	11.360640
15.523636	1056.413291	11.365645
15.235715	1068.184211	11.370650
15.654109	1074.302499	11.375655
15.550806	1065.418444	11.380659
15.566214	1065.755078	11.385664
15.779604	1073.074615	11.390669
15.841814	1074.941357	11.395674
15.577283	1072.144990	11.400679
15.994591	1072.543685	11.405683
15.840663	1067.922441	11.410688
15.963702	1069.710092	11.415693
15.353953	1080.425298	11.420698
15.772806	1068.658793	11.425703
15.943106	1082.331042	11.430707
16.450074	1095.449699	11.435712
16.527904	1092.067277	11.440717
16.374997	1080.988057	11.445722
16.526964	1077.008747	11.450727
16.424040	1079.829101	11.455731
16.569491	1063.621225	11.460736
16.444341	1064.510147	11.465741
16.236844	1067.383447	11.470746
16.270487	1064.648339	11.475751
16.533040	1082.201054	11.480755
16.544980	1089.019704	11.485760
16.983173	1089.703659	11.490765
16.946440	1092.915593	11.495770
16.849609	1077.908590	11.500775
16.545230	1075.320433	11.505779
16.476751	1079.975649	11.510784
16.850307	1087.733287	11.515789
16.765147	1094.332452	11.520794
16.796752	1084.862304	11.525799
16.987737	1091.753327	11.530803
17.085397	1085.338329	11.535808
17.332266	1077.543319	11.540813
17.309331	1089.317726	11.545818
16.951233	1099.362010	11.550823
17.185666	1103.042435	11.555827
17.224642	1090.999809	11.560832
17.107516	1084.641145	11.565837
16.804975	1109.963214	11.570842
17.154745	1103.419687	11.575847
16.958389	1106.601887	11.580851
17.204301	1119.902556	11.585856
17.622382	1122.821179	11.590861
17.587261	1132.184751	11.595866
17.911022	1134.356726	11.600871
17.849869	1127.910266	11.605875
17.520112	1131.847054	11.610880
17.925378	1124.715907	11.615885
17.735855	1126.137087	11.620890
18.082063	1124.995353	11.625895
17.855901	1132.817124	11.630899
17.873989	1125.408671	11.635904
17.605919	1135.336117	11.640909
17.766794	1136.280353	11.645914
17.865614	1123.196007	11.650919
17.812881	1131.005886	11.655923
17.896268	1131.483072	11.660928
18.209307	1127.799768	11.665933
18.169956	1137.433686	11.670938
18.202243	1123.248163	11.675943
18.253825	1126.483867	11.680947
18.264417	1131.662670	11.685952
18.247705	1120.501772	11.690957
18.168975	1132.092718	11.695962
18.786923	1144.061432	11.700967
18.602931	1138.328441	11.705971
18.648803	1152.671904	11.710976
18.902177	1143.620525	11.715981
18.675518	1149.737642	11.720986
18.995767	1146.184075	11.725991
18.839676	1135.012278	11.730995
18.810114	1126.130618	11.736000
18.785487	1119.594755	11.741005
18.637965	1122.452193	11.746010
19.101771	1130.998155	11.751015
19.150757	1146.763572	11.756019
18.974908	1134.831656	11.761024
19.424417	1124.520522	11.766029
18.999637	1138.588940	11.771034
18.987200	1128.316784	11.776039
19.170327	1132.384669	11.781043
19.452220	1142.744818	11.786048
19.361481	1147.972904	11.791053
19.233463	1151.975296	11.796058
19.619207	1138.821520	11.801063
19.617439	1138.170536	11.806067
19.514117	1128.083192	11.811072
19.568639	1115.814920	11.816077
19.367103	1109.649485	11.821082
19.588050	1121.492259	11.826087
19.637451	1135.401466	11.831091
19.487827	1140.214727	11.836096
20.124478	1145.956027	11.841101
19.883895	1153.521479	11.846106
19.981721	1135.807193	11.851111
19.707316	1123.400557	11.856115
19.627076	1139.733796	11.861120
19.853805	1139.131528	11.866125
19.764448	1147.177500	11.871130
19.819678	1148.570686	11.876135
19.685797	1149.177145	11.881139
19.839586	1147.354869	11.886144
20.066665	1147.451158	11.891149
19.866514	1145.325774	11.896154
19.986912	1142.524773	11.901159
20.252256	1160.772599	11.906163
20.360923	1175.747911	11.911168
20.739082	1170.409392	11.916173
20.537046	1183.415696	11.921178
20.332307	1155.087490	11.926183
20.400807	1156.022806	11.931187
20.419499	1172.258299	11.936192
20.698395	1178.567620	11.941197
20.717480	1185.612265	11.946202
20.854762	1181.789816	11.951207
20.819595	1174.033428	11.956211
20.711682	1183.178399	11.961216
20.732490	1179.018124	11.966221
20.606663	1182.154397	11.971226
21.143468	1178.334465	11.976231
20.835500	1186.080998	11.981235
20.753131	1182.309351	11.986240
20.998357	1174.558708	11.991245
20.785686	1181.577232	11.996250
20.990489	1179.819359	12.001255
20.924278	1178.579388	12.006259
20.874968	1177.516501	12.011264
21.061959	1178.188484	12.016269
21.055472	1177.320625	12.021274
21.079001	1194.821709	12.026279
21.117344	1202.156614	12.031283
21.511713	1210.325753	12.036288
21.478380	1213.295889	12.041293
21.274754	1207.837247	12.046298
21.901326	1187.116368	12.051303
21.348484	1187.693449	12.056307
21.149078	1173.385552	12.061312
21.662659	1171.605242	12.066317
21.476213	1188.002784	12.071322
21.409838	1173.503353	12.076327
21.451201	1179.946756	12.081331
21.210089	1176.030111	12.086336
21.689010	1165.370470	12.091341
21.668081	1174.104157	12.096346
21.866061	1166.723765	12.101351
21.881344	1159.883464	12.106355
21.251076	1147.618721	12.111360
21.581673	1136.992218	12.116365
21.225278	1141.981964	12.121370
21.278993	1137.078415	12.126375
21.034630	1139.315768	12.131379
21.066068	1139.922669	12.136384
21.172793	1134.510755	12.141389
21.163858	1144.718587	12.146394
21.465078	1138.081860	12.151399
21.723252	1137.726897	12.156403
21.275028	1141.874976	12.161408
21.691063	1129.495417	12.166413
21.223398	1133.629247	12.171418
21.305616	1134.653840	12.176423
21.289391	1144.854950	12.181427
21.306517	1138.906949	12.186432
21.419506	1133.828362	12.191437
21.271759	1141.934107	12.196442
21.417016	1140.762919	12.201447
21.336203	1149.367365	12.206451
21.285368	1149.386549	12.211456
21.568211	1141.125282	12.216461
21.425799	1146.058824	12.221466
21.640819	1146.011952	12.226471
21.579666	1156.753264	12.231475
21.754378	1158.841778	12.236480
22.093604	1135.142103	12.241485
21.271172	1130.394060	12.246490
21.344216	1123.216548	12.251495
21.329109	1119.445229	12.256499
21.161101	1127.552620	12.261504
21.314311	1111.876479	12.266509
21.082014	1124.073825	12.271514
21.076999	1112.379617	12.276519
21.214894	1114.994408	12.281523
21.108284	1116.027037	12.286528
21.706774	1118.207236	12.291533
21.209090	1122.393160	12.296538
20.946233	1118.271835	12.301543
21.124525	1118.618763	12.306547
21.100073	1125.323382	12.311552
21.243751	1131.455546	12.316557
21.353051	1144.244999	12.321562
21.585217	1144.004575	12.326567
21.385398	1137.689039	12.331571
21.360603	1124.039339	12.336576
21.343939	1115.261287	12.341581
21.385387	1125.259214	12.346586
21.297787	1119.589707	12.351591
21.284449	1125.417317	12.356595
21.456990	1118.515684	12.361600
21.307629	1120.471370	12.366605
20.888071	1130.303121	12.371610
21.099821	1115.563841	12.376615
21.133955	1120.680535	12.381619
21.277737	1122.972680	12.386624
21.443384	1117.920394	12.391629
21.179840	1125.890052	12.396634
21.017454	1131.620007	12.401639
21.289995	1145.104116	12.406643
21.641133	1151.241050	12.411648
21.383873	1130.043025	12.416653
21.493758	1137.035317	12.421658
21.338626	1123.177739	12.426663
21.147224	1128.666308	12.431667
21.083439	1121.294570	12.436672
21.250414	1103.179775	12.441677
21.262134	1122.611327	12.446682
21.151387	1120.088477	12.451687
21.344326	1138.762574	12.456691
21.430130	1139.264607	12.461696
21.515207	1138.413686	12.466701
21.147108	1131.669238	12.471706
21.331381	1126.637633	12.476711
21.111618	1133.349750	12.481715
21.236700	1139.417072	12.486720
21.420220	1125.702606	12.491725
21.734385	1130.150150	12.496730
21.249018	1123.041196	12.501735
21.469647	1124.318111	12.506739
21.647478	1133.959968	12.511744
21.729880	1132.248431	12.516749
21.257291	1131.565302	12.521754
21.520121	1133.978815	12.526759
21.393398	1132.332170	12.531763
21.389999	1129.240246	12.536768
21.512641	1129.182876	12.541773
21.118642	1135.894396	12.546778
21.148940	1132.090600	12.551783
21.262515	1138.402616	12.556787
21.249041	1127.245927	12.561792
21.248887	1132.743421	12.566797
21.193670	1140.630975	12.571802
21.720016	1134.243783	12.576807
21.324515	1140.775767	12.581811
21.242852	1139.617114	12.586816
21.373488	1136.041750	12.591821
21.397604	1139.147792	12.596826
21.386143	1138.447891	12.601831
21.573093	1142.866840	12.606835
21.169125	1127.848844	12.611840
21.160316	1131.724982	12.616845
20.939181	1136.833507	12.621850
21.268522	1140.386050	12.626855
21.409014	1136.611988	12.631859
21.422921	1140.451388	12.636864
21.335266	1139.776255	12.641869
21.281449	1150.454888	12.646874
21.259194	1152.603202	12.651879
21.328317	1153.820702	12.656883
21.635499	1144.290793	12.661888
21.549820	1120.975886	12.666893
20.969365	1124.102651	12.671898
21.154579	1117.643712	12.676903
21.368654	1125.168177	12.681907
21.183865	1128.004751	12.686912
21.327625	1134.013897	12.691917
21.366518	1136.832144	12.696922
21.575651	1133.425617	12.701927
21.208395	1137.682210	12.706931
21.083970	1122.731603	12.711936
21.205586	1132.822408	12.716941
21.432655	1152.583943	12.721946
21.413143	1133.385487	12.726951
21.278518	1126.520223	12.731955
21.334783	1121.436493	12.736960
21.361232	1118.551130	12.741965
21.035334	1111.716379	12.746970
21.398894	1111.309915	12.751975
21.302170	1112.096532	12.756979
21.144040	1110.148961	12.761984
21.177725	1125.770135	12.766989
21.230633	1144.190597	12.771994
21.453990	1137.649870	12.776999
21.416267	1133.765455	12.782003
21.321160	1130.875821	12.787008
21.399214	1107.511167	12.792013
21.202875	1124.164113	12.797018
21.099396	1110.629479	12.802023
21.204845	1125.570559	12.807027
21.212934	1139.453243	12.812032
21.502419	1128.494247	12.817037
21.362955	1133.872030	12.822042
21.436837	1131.564167	12.827047
21.267899	1110.383625	12.832051
20.759131	1120.316332	12.837056
21.350866	1135.184596	12.842061
21.345764	1144.496079	12.847066
21.617624	1135.684615	12.852071
21.221323	1121.326167	12.857075
21.255239	1125.547161	12.862080
21.485591	1109.636362	12.867085
20.942488	1128.613921	12.872090
21.191015	1135.508405	12.877095
21.332918	1128.368795	12.882099
21.163836	1138.103831	12.887104
21.523595	1156.962664	12.892109
21.426609	1149.552051	12.897114
21.630962	1121.463026	12.902119
21.489297	1125.265731	12.907123
21.382685	1121.389153	12.912128
21.709589	1110.217616	12.917133
21.349802	1122.802735	12.922138
21.120895	1127.407856	12.927143
21.183809	1124.527714	12.932147
21.095706	1128.216219	12.937152
21.335513	1127.447858	12.942157
21.144151	1127.965709	12.947162
21.246605	1126.569528	12.952167
21.130584	1128.354312	12.957171
21.107250	1132.136570	12.962176
21.276568	1128.890940	12.967181
21.152960	1133.575466	12.972186
21.129725	1122.473956	12.977191
21.256430	1128.537861	12.982195
21.409185	1135.652629	12.987200
21.331510	1129.678750	12.992205
21.277887	1120.416142	12.997210
21.752844	1126.814024	13.002215
21.641572	1125.086066	13.007219
21.391292	1125.236410	13.012224
21.489804	1123.675273	13.017229
21.352758	1132.757048	13.022234
21.071011	1132.699515	13.027239
21.176738	1127.573201	13.032243
21.391205	1130.819199	13.037248
21.453425	1128.991029	13.042253
21.565327	1128.014401	13.047258
21.381891	1125.116777	13.052263
21.430830	1131.133160	13.057267
21.392176	1122.519466	13.062272
21.758935	1124.634118	13.067277
21.026513	1125.944759	13.072282
21.227331	1125.313507	13.077287
21.545203	1125.370084	13.082291
21.584812	1124.647845	13.087296
21.473195	1118.531145	13.092301
21.144580	1099.849613	13.097306
20.900552	1099.125302	13.102311
21.338366	1112.683161	13.107315
21.220934	1125.199666	13.112320
21.522813	1126.159262	13.117325
21.421651	1136.126323	13.122330
21.163054	1119.410372	13.127335
21.197447	1120.452053	13.132339
21.190646	1128.653587	13.137344
21.649261	1118.063453	13.142349
21.173653	1119.498720	13.147354
21.554809	1110.851195	13.152359
21.166481	1105.286427	13.157363
21.041619	1103.276779	13.162368
21.435855	1104.278416	13.167373
21.272291	1105.652875	13.172378
21.423503	1111.421119	13.177383
21.465420	1104.746912	13.182387
21.306001	1094.929531	13.187392
21.395802	1100.425282	13.192397
21.296524	1118.590066	13.197402
21.229140	1104.392072	13.202407
21.200149	1094.643778	13.207411
21.298736	1104.019913	13.212416
21.354780	1100.496668	13.217421
21.237206	1097.266837	13.222426
21.277247	1090.979301	13.227431
21.119953	1104.955351	13.232435
21.249754	1105.100271	13.237440
21.557470	1092.303556	13.242445
21.048751	1100.932064	13.247450
21.143176	1105.562095	13.252455
21.029986	1111.653214	13.257459
21.096871	1124.857858	13.262464
21.518227	1132.655207	13.267469
21.549625	1139.462892	13.272474
21.515446	1117.929676	13.277479
21.464620	1109.341586	13.282483
21.389388	1115.628509	13.287488
21.530960	1096.711137	13.292493
21.297474	1104.571120	13.297498
21.335901	1100.727399	13.302503
21.528930	1100.848042	13.307507
21.069192	1111.390319	13.312512
21.278369	1105.462167	13.317517
21.248162	1106.151440	13.322522
21.458592	1103.235160	13.327527
21.346184	1102.000986	13.332531
21.059649	1109.198419	13.337536
21.626930	1110.776449	13.342541
21.248538	1113.487773	13.347546
21.262146	1115.324424	13.352551
21.437740	1114.848588	13.357555
21.212835	1113.389497	13.362560
21.417337	1112.087433	13.367565
21.352403	1112.596159	13.372570
21.440287	1112.402401	13.377575
21.410792	1112.012892	13.382579
21.144770	1113.914641	13.387584
21.123802	1110.429696	13.392589
21.256451	1117.309534	13.397594
21.071757	1108.952536	13.402599
21.325187	1103.506197	13.407603
21.404852	1102.258738	13.412608
21.348096	1110.021938	13.417613
21.425846	1120.271122	13.422618
21.533727	1104.513906	13.427623
21.062848	1101.241072	13.432627
21.181392	1119.669959	13.437632
21.208698	1111.802712	13.442637
21.099616	1110.441847	13.447642
20.994288	1110.758313	13.452647
21.251937	1107.515947	13.457651
21.045154	1112.980155	13.462656
21.250814	1107.467314	13.467661
21.162252	1109.395954	13.472666
21.333214	1109.797669	13.477671
21.477237	1119.091660	13.482675
21.296097	1115.170198	13.487680
21.625858	1099.670134	13.492685
21.289941	1105.559434	13.497690
21.048554	1103.287664	13.502695
21.319399	1103.380127	13.507699
21.091484	1110.164499	13.512704
21.430553	1110.030032	13.517709
21.453003	1104.609492	13.522714
21.386589	1111.043244	13.527719
21.157599	1104.722913	13.532723
20.998990	1118.236336	13.537728
21.480287	1118.709986	13.542733
21.440522	1109.323745	13.547738
21.657573	1119.706836	13.552743
21.359759	1115.750364	13.557747
21.226583	1122.653677	13.562752
21.291247	1104.842211	13.567757
21.479366	1113.629257	13.572762
21.569216	1116.597074	13.577767
21.338252	1112.038565	13.582771
21.248255	1117.369027	13.587776
21.276337	1109.553699	13.592781
20.984242	1114.124737	13.597786
21.200450	1122.099883	13.602791
21.211237	1119.615999	13.607795
20.839102	1121.443206	13.612800
21.081927	1118.558028	13.617805
20.870600	1128.452764	13.622810
21.143509	1120.505340	13.627815
21.378736	1121.765734	13.632819
21.186643	1125.846149	13.637824
21.604469	1121.802348	13.642829
21.199455	1121.874865	13.647834
21.419046	1117.358041	13.652839
21.253271	1117.170045	13.657843
21.487818	1120.690391	13.662848
21.592232	1117.552889	13.667853
21.083943	1125.530041	13.672858
21.091657	1127.701958	13.677863
21.211160	1123.803510	13.682867
21.102700	1130.094161	13.687872
21.237553	1126.268960	13.692877
21.177827	1122.569414	13.697882
21.649805	1126.113397	13.702887
21.427623	1124.210733	13.707891
21.163614	1124.290725	13.712896
21.511538	1124.244734	13.717901
21.103540	1130.067479	13.722906
21.571709	1117.279056	13.727911
21.316922	1118.119269	13.732915
21.526379	1122.818483	13.737920
21.906261	1118.556800	13.742925
21.419942	1134.991070	13.747930
21.629146	1129.021902	13.752935
21.481710	1125.606011	13.757939
21.443268	1131.406087	13.762944
21.824466	1119.011592	13.767949
21.258972	1105.607421	13.772954
21.028936	1102.100627	13.777959
21.209473	1110.095648	13.782963
21.190871	1121.443600	13.787968
21.470658	1107.988196	13.792973
21.374402	1105.611275	13.797978
21.279593	1088.762790	13.802983
21.306635	1096.030056	13.807987
21.185824	1091.565953	13.812992
21.274529	1097.495552	13.817997
20.951023	1110.365830	13.823002
21.319396	1113.716593	13.828007
21.438250	1115.714659	13.833011
21.259443	1132.817418	13.838016
21.312622	1122.585265	13.843021
21.523691	1135.891507	13.848026
21.146025	1116.628765	13.853031
21.172717	1107.236658	13.858035
21.284523	1119.913723	13.863040
21.574591	1116.666184	13.868045
21.091426	1108.678497	13.873050
21.388979	1101.455727	13.878055
21.194366	1094.619758	13.883059
21.016344	1117.901847	13.888064
21.071350	1127.001875	13.893069
21.514925	1130.604007	13.898074
21.502767	1133.416203	13.903079
21.494326	1135.508693	13.908083
21.332310	1123.486268	13.913088
21.217592	1104.878640	13.918093
21.133017	1108.132901	13.923098
21.059951	1122.189366	13.928103
21.543161	1124.676542	13.933107
21.201500	1130.673216	13.938112
21.394523	1119.751690	13.943117
21.319494	1134.327313	13.948122
21.714503	1132.930206	13.953127
21.280750	1102.873959	13.958131
21.129395	1110.306883	13.963136
21.483495	1091.081225	13.968141
21.309491	1111.957741	13.973146
21.212955	1105.092720	13.978151
21.213310	1095.085849	13.983155
20.862040	1094.768161	13.988160
21.025159	1108.281515	13.993165
21.438105	1130.049282	13.998170
21.474133	1132.297111	14.003175
21.115546	1132.013705	14.008179
20.895561	1128.013277	14.013184
21.247251	1122.261091	14.018189
21.332637	1133.172695	14.023207
21.146268	1140.336710	14.028224
21.408424	1142.751934	14.033242
21.369734	1136.815419	14.038259
21.635907	1128.245093	14.043277
21.443600	1143.182151	14.048295
21.103286	1149.669960	14.053312
21.282287	1133.556929	14.058330
21.100165	1139.185037	14.063347
21.455670	1133.658335	14.068365
20.971081	1143.191633	14.073383
21.308393	1138.285227	14.078400
21.073458	1132.077214	14.083418
21.253335	1145.256097	14.088435
21.474314	1135.350435	14.093453
21.168361	1143.665283	14.098471
21.315185	1156.710240	14.103488
21.636175	1165.511833	14.108506
21.535377	1165.498060	14.113523
21.878207	1159.582484	14.118541
21.744936	1174.474766	14.123559
21.801093	1169.352075	14.128576
21.709651	1171.082822	14.133594
21.639263	1172.756730	14.138611
22.001396	1160.865453	14.143629
21.913867	1170.139606	14.148647
21.738875	1168.637038	14.153664
21.798712	1144.466516	14.158682
21.746157	1160.761595	14.163699
22.018427	1149.078137	14.168717
21.921993	1151.025176	14.173735
21.725165	1150.764030	14.178752
21.704856	1136.574295	14.183770
21.650876	1157.478432	14.188787
22.194904	1163.929022	14.193805
21.943100	1166.130499	14.198823
22.089057	1157.219901	14.203840
21.781486	1147.164154	14.208858
21.989493	1161.813236	14.213875
21.892580	1166.934635	14.218893
21.881051	1170.058885	14.223911
21.821451	1170.085730	14.228928
22.143310	1169.000984	14.233946
21.712737	1173.845273	14.238963
22.224579	1161.700464	14.243981
22.136716	1171.481171	14.248999
21.902281	1177.985138	14.254016
21.958091	1177.062370	14.259034
22.268109	1168.197958	14.264051
22.176000	1173.389377	14.269069
22.139157	1172.003199	14.274087
22.095687	1170.858745	14.279104
22.298966	1174.302658	14.284122
22.183978	1171.291466	14.289139
22.105125	1179.667640	14.294157
21.779278	1180.155362	14.299175
21.878086	1172.870877	14.304192
22.494346	1166.634844	14.309210
21.963631	1176.239226	14.314227
22.124032	1183.410089	14.319245
22.730541	1204.197943	14.324263
22.469010	1197.865945	14.329280
22.359826	1192.186037	14.334298
22.687120	1193.890901	14.339315
22.508064	1187.522159	14.344333
22.398086	1168.346171	14.349351
22.190590	1175.676377	14.354368
22.363738	1178.231641	14.359386
22.797776	1190.894203	14.364403
22.794292	1191.627807	14.369421
22.530614	1168.952842	14.374439
22.483027	1176.496638	14.379456
22.811545	1168.999345	14.384474
22.740729	1163.972409	14.389491
23.075891	1168.453905	14.394509
22.796760	1171.641282	14.399527
22.558486	1169.264790	14.404544
22.864838	1162.283829	14.409562
22.586503	1172.838936	14.414579
22.858807	1168.455681	14.419597
22.675928	1166.653931	14.424615
22.416321	1163.532102	14.429632
22.686534	1158.641109	14.434650
22.439821	1171.500312	14.439667
22.981552	1188.784428	14.444685
22.995448	1197.477720	14.449703
22.788192	1183.621341	14.454720
22.939286	1177.950263	14.459738
22.910315	1192.807054	14.464755
23.159270	1183.384523	14.469773
22.946678	1189.859845	14.474791
22.714854	1172.809513	14.479808
23.161884	1180.486779	14.484826
23.172993	1197.076905	14.489843
23.177206	1180.025098	14.494861
23.211864	1173.183415	14.499879
22.984778	1164.876561	14.504896
23.244761	1158.341859	14.509914
22.917227	1168.728636	14.514931
23.237557	1166.289795	14.519949
23.027520	1160.320825	14.524967
22.847832	1162.257549	14.529984
23.377989	1186.057234	14.535002
23.272584	1184.447615	14.540019
23.191317	1181.783391	14.545037
23.465639	1178.017994	14.550055
22.957953	1169.870718	14.555072
23.521157	1180.341952	14.560090
23.449595	1176.444534	14.565107
23.056131	1174.048748	14.570125
23.532307	1175.533242	14.575143
23.386136	1170.777865	14.580160
23.140004	1169.281924	14.585178
23.047110	1167.088307	14.590195
23.440487	1181.347632	14.595213
23.569957	1185.171398	14.600231
23.226364	1206.417516	14.605248
23.454068	1194.901574	14.610266
23.600978	1204.144651	14.615283
23.679864	1198.878328	14.620301
24.101301	1198.795421	14.625319
23.485595	1185.293612	14.630336
23.225135	1165.089301	14.635354
23.320207	1191.637177	14.640371
23.427327	1196.255723	14.645389
23.701464	1197.670198	14.650407
23.317283	1204.478051	14.655424
23.429966	1208.016644	14.660442
23.657812	1202.410391	14.665459
23.505337	1204.754904	14.670477
23.705193	1207.265016	14.675495
23.680323	1207.331939	14.680512
23.851565	1198.082237	14.685530
23.810942	1201.196977	14.690547
23.774318	1199.478861	14.695565
23.949723	1202.291739	14.700583
23.734615	1199.104605	14.705600
24.029175	1187.947657	14.710618
23.990602	1198.980484	14.715635
23.870182	1204.196878	14.720653
24.215522	1193.263057	14.725671
23.997446	1204.370134	14.730688
24.225209	1190.316956	14.735706
23.945341	1210.539914	14.740723
23.829887	1202.108271	14.745741
23.924557	1193.748512	14.750759
23.932739	1193.953306	14.755776
24.183874	1189.804649	14.760794
24.029628	1205.854882	14.765811
23.925616	1202.134088	14.770829
24.058121	1194.012108	14.775847
24.156803	1194.270106	14.780864
24.226813	1190.203818	14.785882
24.077599	1194.956051	14.790899
23.869147	1200.055926	14.795917
24.247936	1194.781099	14.800935
23.828794	1195.768181	14.805952
24.296903	1198.457300	14.810970
24.356693	1222.124427	14.815987
24.160720	1221.787640	14.821005
24.519424	1222.449325	14.826023
24.383820	1227.402314	14.831040
24.662684	1213.084567	14.836058
24.248935	1220.595550	14.841075
24.184649	1216.696961	14.846093
24.564074	1219.033721	14.851111
24.446430	1229.841661	14.856128
24.510816	1225.724351	14.861146
24.833875	1220.381327	14.866163
24.529994	1214.521680	14.871181
24.679861	1193.567637	14.876199
24.581959	1203.858042	14.881216
24.674348	1192.830860	14.886234
24.708379	1178.365009	14.891251
24.343139	1195.663226	14.896269
24.617718	1207.434183	14.901287
24.285832	1207.263787	14.906304
24.594347	1214.157792	14.911322
25.019959	1218.777459	14.916339
24.537332	1217.968875	14.921357
24.838265	1214.306189	14.926375
25.009349	1227.342621	14.931392
25.021217	1223.188071	14.936410
25.070395	1222.516463	14.941427
24.562810	1210.531052	14.946445
25.096733	1191.892545	14.951463
25.038821	1197.931078	14.956480
24.943363	1197.170857	14.961498
24.810778	1190.198540	14.966515
24.671036	1191.622395	14.971533
24.816333	1205.760866	14.976551
24.428533	1218.048021	14.981568
24.829242	1216.305771	14.986586
24.579014	1221.011204	14.991603
24.506264	1217.689679	14.996621
24.802663	1217.222456	15.001639
24.554878	1225.575263	15.006656
24.805193	1241.041926	15.011674
25.433161	1251.381763	15.016691
25.323401	1267.390362	15.021709
25.312873	1257.976134	15.026727
25.375387	1254.246072	15.031744
25.468412	1248.379738	15.036762
25.331545	1228.298769	15.041779
25.227653	1224.393911	15.046797
25.662565	1232.071565	15.051815
25.186095	1220.705660	15.056832
25.068176	1211.108820	15.061850
25.355773	1227.653312	15.066867
25.193706	1242.079932	15.071885
25.235246	1240.734728	15.076903
25.184735	1253.932365	15.081920
25.360142	1253.070741	15.086938
25.432776	1251.154299	15.091955
25.291657	1252.213446	15.096973
25.694247	1247.625348	15.101991
25.842542	1255.999945	15.107008
25.662242	1241.711356	15.112026
26.007820	1246.345369	15.117043
25.718061	1250.928130	15.122061
26.023244	1239.605858	15.127079
25.529431	1228.794832	15.132096
25.694060	1211.195172	15.137114
25.630277	1213.881036	15.142131
25.371924	1219.872896	15.147149
25.644926	1224.238484	15.152167
25.931456	1244.852492	15.157184
25.845842	1242.648265	15.162202
25.757761	1229.483827	15.167219
25.801544	1233.313406	15.172237
25.909510	1240.327497	15.177255
25.629238	1223.188879	15.182272
25.727416	1221.762287	15.187290
26.191432	1244.136477	15.192307
25.845379	1245.829190	15.197325
26.064049	1229.635009	15.202343
26.047551	1245.188273	15.207360
25.882367	1242.290462	15.212378
25.798786	1219.858821	15.217395
25.603508	1235.612043	15.222413
26.126672	1236.955347	15.227431
26.183718	1246.409407	15.232448
26.131172	1228.396059	15.237466
26.223941	1240.065480	15.242483
25.733455	1249.932475	15.247501
26.123483	1244.783250	15.252519
26.175695	1240.740235	15.257536
26.072777	1248.830857	15.262554
26.077488	1244.498121	15.267571
26.026193	1247.859959	15.272589
26.195820	1249.634021	15.277607
26.315099	1251.755878	15.282624
26.276597	1243.082282	15.287642
26.393247	1240.614566	15.292659
26.090024	1241.101828	15.297677
26.247281	1239.571432	15.302695
26.380747	1233.671914	15.307712
26.065737	1247.117790	15.312730
26.400461	1266.973826	15.317747
26.665615	1278.335792	15.322765
26.632104	1268.223667	15.327783
26.547698	1273.986464	15.332800
26.430840	1272.578431	15.337818
26.650743	1263.092843	15.342835
26.582111	1270.676224	15.347853
26.698976	1264.208344	15.352871
26.940041	1267.975009	15.357888
26.651586	1264.456644	15.362906
27.068215	1261.875017	15.367923
26.860467	1245.078731	15.372941
26.751523	1237.803752	15.377959
26.534788	1248.097411	15.382976
26.604483	1251.859943	15.387994
26.651807	1246.650545	15.393011
26.624811	1264.635778	15.398029
27.026548	1263.796258	15.403047
26.898572	1269.435443	15.408064
26.844244	1267.594302	15.413082
27.300653	1265.980014	15.418099
27.048136	1271.697263	15.423117
27.277972	1248.388197	15.428135
27.015186	1242.718609	15.433152
27.151925	1231.860499	15.438170
27.153573	1239.516023	15.443187
26.954837	1242.135328	15.448205
26.809671	1230.950952	15.453223
26.951031	1248.610447	15.458240
26.986776	1243.796144	15.463258
27.125005	1258.851276	15.468275
26.914340	1267.295712	15.473293
26.892452	1272.644278	15.478311
27.345510	1271.208272	15.483328
27.277316	1269.554957	15.488346
27.208572	1255.261147	15.493363
27.300187	1277.252770	15.498381
27.385419	1273.397958	15.503399
27.588517	1267.328449	15.508416
27.283450	1268.155772	15.513434
27.573180	1260.655180	15.518451
27.274178	1279.237506	15.523469
27.354538	1271.740413	15.528487
27.384308	1264.957667	15.533504
27.364982	1267.649035	15.538522
27.577842	1256.586861	15.543539
27.485584	1275.471257	15.548557
27.566290	1279.697647	15.553575
27.511474	1263.897823	15.558592
27.252757	1277.783054	15.563610
27.699365	1276.324481	15.568627
27.361142	1273.496732	15.573645
27.708635	1265.437950	15.578663
27.633620	1280.242401	15.583680
27.255804	1271.264260	15.588698
27.682701	1264.150769	15.593715
27.817317	1292.029569	15.598733
27.806593	1300.058325	15.603751
27.855552	1291.147386	15.608768
27.889531	1298.808796	15.613786
27.984454	1282.719233	15.618803
27.787976	1275.791671	15.623821
27.920648	1282.119161	15.628839
28.133416	1290.796522	15.633856
28.054198	1294.820338	15.638874
27.804271	1273.340066	15.643891
27.900492	1283.454853	15.648909
27.862174	1291.650024	15.653927
28.214248	1285.226418	15.658944
28.251747	1303.476688	15.663962
28.292607	1288.465381	15.668979
28.290886	1296.325962	15.673997
28.256424	1281.531164	15.679015
28.287582	1272.645097	15.684032
28.007647	1269.685358	15.689050
28.247430	1258.250808	15.694067
28.203144	1277.937649	15.699085
28.317654	1278.715360	15.704103
28.191553	1283.961002	15.709120
28.075846	1296.728637	15.714138
28.557326	1292.654898	15.719155
28.492212	1298.581365	15.724173
28.453065	1290.884675	15.729191
28.391016	1308.089054	15.734208
28.605054	1297.695186	15.739226
28.692566	1289.161910	15.744243
28.200159	1303.150501	15.749261
28.445469	1299.265433	15.754279
28.473527	1288.953141	15.759296
28.542871	1298.147302	15.764314
28.966659	1290.851826	15.769331
28.517613	1299.156551	15.774349
28.402965	1280.924957	15.779367
28.494820	1292.756585	15.784384
28.140291	1302.383286	15.789402
28.531437	1293.101599	15.794419
28.448485	1283.186107	15.799437
28.366377	1305.062336	15.804455
28.437313	1303.271999	15.809472
28.415181	1313.887019	15.814490
28.890732	1318.799197	15.819507
28.917424	1327.702882	15.824525
28.891720	1324.134733	15.829543
29.049715	1323.941261	15.834560
28.861208	1324.529778	15.839578
29.286339	1320.101655	15.844595
29.235587	1315.290113	15.849613
29.218494	1317.045199	15.854631
29.299056	1315.368153	15.859648
28.945085	1295.976083	15.864666
29.123918	1299.729087	15.869683
29.125292	1300.450911	15.874701
29.228394	1300.141928	15.879719
29.639289	1302.586940	15.884736
29.230826	1303.290758	15.889754
29.106774	1279.707751	15.894771
28.978303	1295.892396	15.899789
29.097788	1300.156652	15.904807
29.166717	1303.856400	15.909824
29.151513	1302.749898	15.914842
29.486548	1297.651896	15.919859
29.499779	1301.229968	15.924877
29.118864	1312.861737	15.929895
29.355306	1312.618003	15.934912
29.387299	1311.041511	15.939930
29.095899	1315.649722	15.944947
29.533733	1310.348134	15.949965
29.370042	1322.327506	15.954983
29.271720	1316.103131	15.960000
29.147228	1317.685012	15.965018
29.638210	1307.792799	15.970035
29.318856	1319.237007	15.975053
29.417574	1335.368160	15.980071
29.709065	1341.129234	15.985088
29.966766	1340.521891	15.990106
29.764116	1330.691524	15.995123
29.822352	1335.896775	16.000141
30.209404	1335.275095	16.005159
30.008466	1322.850579	16.010176
29.735929	1324.599215	16.015194
29.883736	1299.424986	16.020211
29.817966	1313.693177	16.025229
29.828146	1332.916808	16.030247
30.136967	1340.592609	16.035264
29.802985	1347.252524	16.040282
29.933036	1345.306464	16.045299
30.242558	1333.547705	16.050317
29.966929	1344.879569	16.055335
30.163345	1350.166606	16.060352
30.046836	1346.999892	16.065370
30.168100	1348.569323	16.070387
30.287554	1335.733481	16.075405
30.248523	1340.107971	16.080423
30.475747	1324.437703	16.085440
30.260625	1344.527827	16.090458
30.286901	1334.465894	16.095475
30.381851	1335.485824	16.100493
30.444283	1322.084942	16.105511
30.188985	1307.510951	16.110528
30.132754	1317.124694	16.115546
30.436381	1327.771140	16.120563
30.863752	1338.328648	16.125581
30.343933	1342.394431	16.130599
30.470248	1324.064579	16.135616
30.322746	1339.684454	16.140634
30.509424	1321.757105	16.145651
30.500454	1336.927028	16.150669
30.129487	1343.279813	16.155687
30.529357	1333.037177	16.160704
30.408132	1323.543035	16.165722
30.413278	1332.022302	16.170739
30.433353	1339.929767	16.175757
30.536030	1339.041985	16.180775
30.693688	1324.664809	16.185792
30.646092	1338.341823	16.190810
30.671498	1349.194677	16.195827
30.821188	1359.138970	16.200845
30.767021	1372.974365	16.205863
31.033283	1361.846966	16.210880
31.066997	1360.112894	16.215898
30.799655	1372.358946	16.220915
31.424382	1358.258027	16.225933
31.039982	1360.463376	16.230951
31.024831	1348.253023	16.235968
30.816617	1366.448179	16.240986
30.866400	1361.189585	16.246003
31.117678	1349.495158	16.251021
31.179168	1366.917427	16.256039
31.089842	1356.858185	16.261056
31.051057	1358.410672	16.266074
31.249675	1355.464255	16.271091
31.355289	1361.149591	16.276109
30.983004	1363.371884	16.281127
31.276679	1349.907356	16.286144
31.100948	1354.405897	16.291162
31.032616	1357.855420	16.296179
31.348507	1360.947941	16.301197
31.094413	1356.794872	16.306215
31.153212	1351.349229	16.311232
31.120159	1363.814308	16.316250
31.500051	1377.720480	16.321267
31.564413	1383.443864	16.326285
31.378125	1385.564138	16.331303
31.730196	1379.159368	16.336320
31.729019	1394.770123	16.341338
31.532849	1399.613281	16.346355
32.012344	1381.418937	16.351373
31.812488	1368.575789	16.356391
31.894162	1356.642567	16.361408
32.141786	1348.038105	16.366426
31.784930	1355.050879	16.371443
31.976648	1351.536136	16.376461
31.941862	1351.928680	16.381479
32.080934	1349.790847	16.386496
32.068346	1349.619861	16.391514
31.587891	1367.528106	16.396531
31.809434	1351.894894	16.401549
31.858553	1354.990635	16.406567
32.104081	1326.289829	16.411584
32.035869	1373.652881	16.416602
31.903418	1346.868464	16.421619
32.146173	1352.989669	16.426637
32.179992	1360.896526	16.431655
32.220963	1345.716830	16.436672
32.195591	1342.869059	16.441690
32.225000	1343.982811	16.446707
32.294494	1350.504449	16.451725
32.150273	1355.027852	16.456743
32.356869	1348.569219	16.461760
32.361489	1348.047856	16.466778
32.110909	1352.040815	16.471795
32.500735	1365.599331	16.476813
32.374019	1386.468208	16.481831
32.650025	1381.406333	16.486848
32.946630	1374.529071	16.491866
32.650813	1364.996679	16.496883
32.497009	1342.393578	16.501901
32.169547	1346.513627	16.506919
32.212300	1348.232431	16.511936
32.393858	1373.587096	16.516954
32.374393	1381.386059	16.521971
32.981835	1373.886649	16.526989
32.595718	1370.113276	16.532007
32.602858	1376.797452	16.537024
32.855173	1380.685048	16.542042
32.627011	1385.004773	16.547059
33.160521	1376.839186	16.552077
32.797133	1387.621942	16.557095
32.897750	1375.158726	16.562112
32.681037	1375.605453	16.567130
32.582278	1389.636737	16.572147
32.938660	1368.130413	16.577165
32.696516	1377.712498	16.582183
32.701042	1379.783464	16.587200
32.901352	1379.175834	16.592218
32.621882	1374.271763	16.597235
32.959800	1374.615879	16.602253
33.258554	1397.556206	16.607271
33.222272	1386.741305	16.612288
33.269965	1390.774793	16.617306
32.816352	1403.527200	16.622323
33.570866	1392.444605	16.627341
33.417074	1406.566478	16.632359
33.392445	1389.119481	16.637376
33.510942	1375.288042	16.642394
33.573647	1399.445773	16.647411
33.551234	1376.190888	16.652429
33.229805	1374.840639	16.657447
33.219019	1374.389370	16.662464
33.536664	1382.181762	16.667482
33.167992	1407.092561	16.672499
33.464511	1399.123632	16.677517
33.105185	1402.525193	16.682535
33.594724	1402.190757	16.687552
33.646171	1400.537222	16.692570
33.388386	1410.543389	16.697587
33.381721	1405.073560	16.702605
33.307958	1406.952524	16.707623
33.442403	1403.253422	16.712640
33.645781	1411.473036	16.717658
33.474314	1432.778548	16.722675
33.962262	1433.633563	16.727693
33.864877	1438.231319	16.732711
34.030036	1434.541468	16.737728
34.074439	1439.885815	16.742746
34.183436	1434.325171	16.747763
34.341915	1426.058920	16.752781
34.121421	1434.681198	16.757799
34.486379	1402.637419	16.762816
34.453794	1397.244085	16.767834
34.038702	1409.192837	16.772851
34.441901	1389.023940	16.777869
34.366106	1397.656152	16.782887
34.056614	1401.488636	16.787904
34.225983	1375.497590	16.792922
34.078817	1404.077489	16.797939
34.113283	1396.306082	16.802957
34.203580	1392.131111	16.807975
34.229480	1385.089379	16.812992
34.503974	1389.673429	16.818010
34.224819	1389.186310	16.823027
34.464839	1394.557644	16.828045
34.545088	1387.235113	16.833063
34.716569	1382.542262	16.838080
34.758527	1386.691494	16.843098
34.443023	1395.958105	16.848115
34.647206	1398.060151	16.853133
34.466810	1386.348023	16.858151
34.256373	1393.205331	16.863168
34.460196	1416.675203	16.868186
34.406381	1427.525019	16.873203
34.865579	1408.251647	16.878221
34.676250	1421.097199	16.883239
34.665495	1435.296961	16.888256
35.026185	1419.520363	16.893274
35.110464	1417.117555	16.898291
35.290516	1415.361711	16.903309
35.228556	1428.753241	16.908327
35.182368	1418.248206	16.913344
35.353216	1419.414912	16.918362
35.174573	1416.067757	16.923379
35.046500	1389.995135	16.928397
34.680257	1398.970968	16.933415
34.772527	1407.730538	16.938432
35.145431	1418.768695	16.943450
34.836747	1425.050234	16.948467
35.292195	1420.035233	16.953485
35.276675	1420.632344	16.958503
34.899538	1422.839688	16.963520
35.251284	1414.490713	16.968538
35.060754	1414.456643	16.973555
35.321910	1411.080248	16.978573
35.279107	1417.492411	16.983591
35.275671	1418.153661	16.988608
35.572741	1420.380896	16.993626
35.457940	1439.116518	16.998643
35.685348	1429.305585	17.003661
35.552475	1428.876932	17.008679
35.821260	1445.789614	17.013696
35.839787	1431.546205	17.018714
35.472106	1427.997963	17.023731
35.662153	1435.598376	17.028749
35.972849	1449.028019	17.033767
35.924078	1436.311725	17.038784
35.826634	1422.624791	17.043802
35.408031	1432.537071	17.048819
35.779711	1433.184115	17.053837
36.047011	1441.322766	17.058855
36.101429	1441.293675	17.063872
36.297210	1442.656179	17.068890
35.841003	1444.624455	17.073907
36.035822	1424.170994	17.078925
36.152900	1459.040233	17.083943
35.950010	1444.659092	17.088960
36.229408	1444.266934	17.093978
35.861958	1456.291496	17.098995
36.155286	1450.717178	17.104013
36.111932	1450.615592	17.109031
36.084786	1441.878717	17.114048
36.126532	1450.025030	17.119066
35.884706	1448.092647	17.124083
36.029878	1450.193102	17.129101
35.862116	1429.133646	17.134119
35.783983	1449.881610	17.139136
36.426686	1474.722464	17.144154
36.354300	1463.488548	17.149171
36.368941	1471.057179	17.154189
36.748256	1462.588949	17.159207
36.517456	1480.696615	17.164224
36.651931	1467.158268	17.169242
36.414868	1478.830148	17.174259
36.675816	1472.098526	17.179277
36.861517	1466.687656	17.184295
36.711077	1484.299595	17.189312
36.976769	1469.156290	17.194330
36.957607	1486.294266	17.199347
36.785837	1477.429425	17.204365
36.601964	1477.104858	17.209383
36.683883	1481.952456	17.214400
37.461525	1461.585317	17.219418
37.199995	1467.455088	17.224435
36.992400	1471.224148	17.229453
36.963137	1468.145739	17.234471
36.817087	1460.733421	17.239488
37.024372	1463.041048	17.244506
36.816580	1469.559771	17.249523
36.812462	1466.354657	17.254541
37.090036	1468.728153	17.259559
37.086919	1479.930144	17.264576
37.230540	1490.506276	17.269594
37.109239	1495.815723	17.274611
37.408355	1492.500895	17.279629
37.495188	1492.353378	17.284647
37.115968	1489.132575	17.289664
37.517506	1503.342156	17.294682
37.462209	1490.713371	17.299699
37.711598	1489.248480	17.304717
37.825464	1487.339589	17.309735
37.392909	1497.559305	17.314752
37.988786	1484.345331	17.319770
37.663067	1495.603502	17.324787
37.515147	1500.822815	17.329805
37.919212	1492.831964	17.334823
37.800635	1498.911757	17.339840
38.067999	1491.037091	17.344858
37.854328	1504.010866	17.349875
37.703029	1489.851113	17.354893
37.406679	1494.582864	17.359911
37.370769	1500.350600	17.364928
37.892867	1505.829573	17.369946
37.998642	1505.156792	17.374963
37.870960	1496.859060	17.379981
38.079551	1498.416155	17.384999
37.514823	1500.664439	17.390016
37.909734	1493.069876	17.395034
38.001457	1518.585413	17.400051
38.146283	1517.539889	17.405069
38.288419	1520.568922	17.410087
38.355509	1523.388127	17.415104
38.728238	1515.108107	17.420122
38.308690	1522.764886	17.425139
38.276179	1524.607399	17.430157
38.324639	1523.806904	17.435175
38.264287	1520.060189	17.440192
38.474483	1510.612168	17.445210
38.583375	1519.914993	17.450227
38.585480	1517.080109	17.455245
38.702713	1518.643910	17.460263
38.292550	1532.904320	17.465280
38.739457	1510.227178	17.470298
38.605459	1512.722948	17.475315
38.480544	1518.607132	17.480333
38.802276	1509.202672	17.485351
38.561371	1516.890733	17.490368
38.735569	1519.113984	17.495386
38.401854	1530.235031	17.500403
38.666784	1526.049474	17.505421
39.110940	1518.565022	17.510439
38.747700	1522.973969	17.515456
38.665985	1533.221127	17.520474
39.197845	1550.867478	17.525491
39.145586	1550.781468	17.530509
39.311110	1551.448811	17.535527
39.252883	1544.483340	17.540544
39.574613	1528.959802	17.545562
39.146687	1539.505997	17.550579
39.038229	1522.904338	17.555597
39.550471	1528.628710	17.560615
39.342430	1537.967935	17.565632
39.740971	1529.781318	17.570650
39.395156	1520.033427	17.575667
39.159055	1513.093192	17.580685
39.879729	1531.289852	17.585703
39.683642	1517.616986	17.590720
39.508855	1507.193744	17.595738
39.430530	1512.304434	17.600755
39.162866	1523.789322	17.605773
39.606622	1523.039043	17.610791
39.290429	1541.904443	17.615808
39.837041	1545.776610	17.620826
39.738887	1539.284698	17.625843
39.770522	1543.154049	17.630861
39.936313	1532.393329	17.635879
39.776421	1548.397649	17.640896
39.904310	1536.269719	17.645914
39.858062	1540.551039	17.650931
39.731722	1546.141306	17.655949
39.886292	1542.583678	17.660967
39.920101	1549.282557	17.665984
39.701765	1542.372509	17.671002
39.913440	1544.160351	17.676019
39.892741	1548.928382	17.681037
40.236678	1552.431753	17.686055
40.205658	1563.037362	17.691072
40.381315	1564.278819	17.696090
40.377004	1577.288484	17.701107
40.444139	1566.567067	17.706125
40.483268	1541.933568	17.711143
40.163590	1539.129548	17.716160
40.445547	1552.022750	17.721178
40.514584	1560.468367	17.726195
40.579770	1558.825206	17.731213
40.743773	1556.900446	17.736231
40.608476	1572.386490	17.741248
40.554491	1563.891350	17.746266
41.008288	1574.882120	17.751283
40.715575	1576.542766	17.756301
40.991395	1564.438411	17.761319
40.648258	1556.753880	17.766336
40.747340	1552.750495	17.771354
41.020939	1547.685801	17.776371
40.734633	1561.687386	17.781389
40.901347	1558.104222	17.786407
40.891785	1569.272704	17.791424
41.082243	1567.686643	17.796442
40.873005	1573.936655	17.801459
40.878154	1573.838344	17.806477
41.008303	1564.410919	17.811495
41.029756	1577.583217	17.816512
40.961013	1566.951110	17.821530
41.162988	1563.838948	17.826547
40.974392	1563.312211	17.831565
41.056404	1561.897602	17.836583
40.720221	1568.175723	17.841600
41.181883	1581.949503	17.846618
41.148117	1577.117861	17.851635
41.207126	1597.082818	17.856653
41.574592	1593.115271	17.861671
41.466499	1590.656598	17.866688
41.247712	1591.773772	17.871706
41.507154	1583.662791	17.876723
41.265060	1580.896726	17.881741
41.439846	1581.008889	17.886759
41.482687	1591.173302	17.891776
42.114772	1607.647562	17.896794
42.011631	1601.359338	17.901811
41.941966	1595.797237	17.906829
41.971291	1586.017789	17.911847
41.534443	1579.447739	17.916864
41.610731	1581.807737	17.921882
42.068483	1595.387098	17.926899
42.218567	1604.755768	17.931917
42.050839	1624.053777	17.936935
42.143225	1617.948296	17.941952
42.208061	1610.711481	17.946970
42.811277	1603.560271	17.951987
41.827537	1598.776303	17.957005
42.136918	1588.497584	17.962023
42.238330	1598.114686	17.967040
42.394290	1605.929839	17.972058
42.443230	1600.727921	17.977075
42.421443	1604.695472	17.982093
42.734069	1611.551262	17.987111
42.545560	1613.338440	17.992128
42.566622	1603.829286	17.997146
42.875169	1603.391578	18.002163
42.084776	1603.316318	18.007181
42.543990	1603.659974	18.012199
42.617233	1605.734170	18.017216
42.382768	1617.128893	18.022234
42.593978	1614.727832	18.027251
42.685474	1612.421369	18.032269
42.741112	1612.996129	18.037287
42.811012	1612.786816	18.042304
42.877873	1601.258452	18.047322
42.920265	1601.078695	18.052339
42.636715	1612.122590	18.057357
42.626119	1606.483425	18.062375
42.844053	1618.394314	18.067392
42.877830	1623.918177	18.072410
43.121425	1626.349029	18.077427
42.870332	1640.887771	18.082445
43.183978	1631.500252	18.087463
43.275746	1633.681611	18.092480
43.371386	1636.120330	18.097498
43.322828	1623.076646	18.102515
43.288582	1631.219450	18.107533
43.623584	1625.001341	18.112551
43.711058	1633.687880	18.117568
43.553608	1632.512802	18.122586
43.757985	1624.542715	18.127603
43.336956	1627.070123	18.132621
43.906310	1629.582731	18.137639
44.007029	1623.103110	18.142656
43.392812	1625.573236	18.147674
43.942681	1623.311649	18.152691
43.800337	1622.521129	18.157709
43.906117	1629.197555	18.162727
43.645281	1625.421437	18.167744
43.658465	1622.949709	18.172762
43.939775	1623.361063	18.177779
43.701574	1626.938414	18.182797
44.031062	1611.926360	18.187815
43.813064	1632.667002	18.192832
43.954612	1639.046718	18.197850
44.245317	1627.674545	18.202867
44.102955	1648.960002	18.207885
44.481893	1654.571977	18.212903
44.445598	1651.120268	18.217920
44.341944	1640.706034	18.222938
44.396001	1628.978341	18.227955
44.122182	1632.622722	18.232973
44.616254	1642.634986	18.237991
44.558614	1656.823566	18.243008
44.391947	1657.361420	18.248026
44.758494	1662.149530	18.253043
44.687326	1660.087653	18.258061
44.522339	1655.629273	18.263079
44.555823	1656.699928	18.268096
44.660301	1659.223758	18.273114
44.624094	1655.638326	18.278131
44.644046	1663.736324	18.283149
44.629579	1656.611235	18.288167
44.686892	1654.649993	18.293184
44.529509	1653.371082	18.298202
44.881223	1645.110071	18.303219
44.600485	1649.436684	18.308237
44.806207	1646.781662	18.313255
45.156496	1667.629928	18.318272
44.996279	1665.744275	18.323290
45.294745	1668.339418	18.328307
45.162048	1671.305345	18.333325
45.462322	1673.612335	18.338343
45.515122	1661.340545	18.343360
45.235073	1673.195615	18.348378
45.534708	1671.571683	18.353395
45.563577	1662.484393	18.358413
45.803954	1671.022300	18.363431
45.772476	1662.721715	18.368448
45.729190	1649.038514	18.373466
45.819230	1637.915413	18.378483
45.306371	1641.146457	18.383501
45.619469	1642.399035	18.388519
46.090632	1650.379450	18.393536
45.385348	1649.942975	18.398554
45.994026	1643.113347	18.403571
45.756017	1656.194960	18.408589
45.678549	1660.001517	18.413607
46.068695	1649.864033	18.418624
46.035443	1658.950516	18.423642
46.038173	1661.293944	18.428659
46.040230	1664.655235	18.433677
45.887602	1663.518711	18.438695
45.882417	1654.580003	18.443712
45.811371	1657.232500	18.448730
45.955696	1652.057824	18.453747
45.988048	1651.167083	18.458765
46.173455	1660.921843	18.463783
46.360004	1656.695266	18.468800
45.921009	1659.481948	18.473818
46.388141	1668.671109	18.478835
46.333187	1694.715294	18.483853
46.370719	1683.526599	18.488871
46.462789	1679.129464	18.493888
46.513764	1679.421823	18.498906
46.781792	1680.366985	18.503923
46.606898	1679.891541	18.508941
46.616886	1670.012872	18.513959
46.597044	1678.379923	18.518976
46.570573	1683.317235	18.523994
46.804611	1668.389558	18.529011
46.836507	1671.865644	18.534029
46.779603	1683.713451	18.539047
46.861911	1672.056723	18.544064
46.532473	1677.891791	18.549082
46.842508	1685.013873	18.554099
47.366708	1703.292423	18.559117
47.249731	1688.560706	18.564135
47.503171	1700.587125	18.569152
47.206446	1713.203094	18.574170
47.707004	1692.580946	18.579187
47.534527	1703.140003	18.584205
47.513761	1706.783372	18.589223
47.871230	1691.040029	18.594240
47.214666	1682.920917	18.599258
47.583599	1671.855561	18.604275
47.754283	1678.196041	18.609293
47.743962	1681.938413	18.614311
47.643886	1664.872779	18.619328
47.567909	1670.094836	18.624346
47.638422	1678.760512	18.629363
47.867790	1688.059963	18.634381
47.704159	1695.016915	18.639399
47.896536	1697.888534	18.644416
47.598375	1694.305541	18.649434
47.790703	1689.901852	18.654451
48.049422	1691.480862	18.659469
47.776018	1698.159589	18.664487
47.762414	1693.401773	18.669504
47.568805	1689.429297	18.674522
48.248226	1700.377890	18.679539
48.243049	1714.701307	18.684557
48.461660	1726.826112	18.689575
48.651623	1721.107726	18.694592
48.414553	1707.033798	18.699610
48.360338	1701.332337	18.704627
48.394380	1706.456636	18.709645
48.380485	1718.064803	18.714663
48.704308	1725.128077	18.719680
48.845820	1721.770692	18.724698
48.795091	1703.437135	18.729715
48.753983	1687.675561	18.734733
48.528677	1691.302781	18.739751
48.660149	1694.582092	18.744768
48.411736	1713.619378	18.749786
48.549712	1721.744205	18.754803
48.699820	1726.186177	18.759821
48.737544	1722.058821	18.764839
48.984736	1727.630488	18.769856
48.621508	1724.628879	18.774874
49.010294	1719.014068	18.779891
49.175403	1725.229614	18.784909
48.572688	1727.386459	18.789927
49.099855	1719.128886	18.794944
49.204147	1745.215407	18.799962
49.219050	1741.365395	18.804979
49.635013	1752.151547	18.809997
49.244356	1742.931335	18.815015
49.448781	1737.352210	18.820032
49.398239	1740.784829	18.825050
49.618456	1738.229727	18.830067
49.599059	1737.347233	18.835085
49.609111	1740.847268	18.840103
50.096258	1734.431814	18.845120
49.643650	1733.324248	18.850138
49.443225	1744.575213	18.855155
49.618096	1732.324794	18.860173
49.619760	1738.733155	18.865191
49.650467	1736.662886	18.870208
49.690609	1742.346229	18.875226
49.799263	1744.674351	18.880243
50.151657	1761.128898	18.885261
50.047535	1767.341780	18.890279
50.110915	1753.742144	18.895296
50.152908	1772.546001	18.900314
50.403067	1769.951511	18.905331
50.435982	1766.985821	18.910349
50.418455	1765.720776	18.915367
50.632361	1754.354459	18.920384
50.659974	1761.872410	18.925402
50.462086	1750.902107	18.930419
50.529849	1746.585908	18.935437
50.505141	1764.775893	18.940455
51.051545	1746.984137	18.945472
50.617382	1746.100146	18.950490
50.543247	1752.202845	18.955507
50.727636	1740.234051	18.960525
50.642514	1758.084446	18.965543
50.926930	1757.488559	18.970560
50.685843	1756.844341	18.975578
50.739503	1770.222466	18.980595
50.793862	1761.714650	18.985613
50.567938	1763.822422	18.990631
50.981176	1750.569695	18.995648
50.905359	1753.095553	19.000666
50.901065	1758.730933	19.005683
51.445275	1768.766752	19.010701
51.188124	1772.859974	19.015719
51.335359	1771.861240	19.020736
51.304063	1769.407592	19.025754
51.309353	1781.346235	19.030771
51.390330	1783.960354	19.035789
51.326727	1797.382373	19.040807
51.599273	1780.471114	19.045824
51.376328	1800.113222	19.050842
51.402016	1799.522414	19.055859
51.715160	1797.051585	19.060877
51.622804	1787.886020	19.065895
51.732983	1781.780778	19.070912
51.915156	1790.323320	19.075930
51.658095	1783.254160	19.080947
52.003528	1778.412316	19.085965
51.954695	1779.253858	19.090983
52.052791	1774.306739	19.096000
51.904777	1779.644144	19.101018
51.893021	1776.984455	19.106035
51.995360	1788.884032	19.111053
52.164631	1812.075334	19.116071
52.267995	1796.696450	19.121088
52.230994	1811.460773	19.126106
52.425954	1815.330893	19.131123
52.682894	1803.693403	19.136141
52.275317	1812.745294	19.141159
52.869927	1797.877962	19.146176
52.678769	1797.530951	19.151194
52.272857	1805.284804	19.156211
52.682581	1803.489142	19.161229
52.807259	1804.817403	19.166247
52.933946	1793.302941	19.171264
52.577111	1794.074050	19.176282
52.638827	1802.596482	19.181299
52.962066	1793.410255	19.186317
52.545603	1790.198468	19.191335
52.629637	1793.082665	19.196352
52.629622	1806.935007	19.201370
52.978346	1826.512726	19.206387
53.334389	1825.202258	19.211405
52.912744	1829.840837	19.216423
53.221908	1828.504811	19.221440
53.163964	1827.225756	19.226458
53.241579	1821.460752	19.231475
53.290761	1812.223835	19.236493
53.337142	1832.957208	19.241511
53.205183	1816.415589	19.246528
53.444423	1830.374520	19.251546
53.112274	1846.416076	19.256563
53.783770	1853.491611	19.261581
53.892010	1850.326697	19.266599
54.164849	1846.455973	19.271616
54.067984	1846.568987	19.276634
54.134643	1845.155227	19.281651
54.235423	1814.091787	19.286669
53.867512	1825.514245	19.291687
53.923278	1813.652421	19.296704
54.137189	1818.213237	19.301722
53.827844	1819.302396	19.306739
54.302798	1820.359290	19.311757
54.298033	1837.734489	19.316775
54.482621	1840.171643	19.321792
54.345465	1826.603919	19.326810
54.089217	1846.471628	19.331827
54.540352	1822.366564	19.336845
54.187139	1840.918924	19.341863
54.208302	1852.084297	19.346880
54.563207	1839.027987	19.351898
54.273164	1832.920481	19.356915
54.484656	1853.397887	19.361933
54.765348	1838.855861	19.366951
54.865644	1840.378353	19.371968
54.502673	1832.062894	19.376986
54.518634	1841.309960	19.382003
55.012493	1838.228273	19.387021
54.879489	1856.344406	19.392039
54.826790	1870.392404	19.397056
55.174612	1863.170112	19.402074
54.793048	1865.872166	19.407091
55.072443	1865.547643	19.412109
55.230755	1875.947104	19.417127
55.138776	1871.105771	19.422144
55.175697	1854.721225	19.427162
55.182571	1861.811516	19.432179
55.384369	1867.577670	19.437197
55.388439	1862.990016	19.442215
55.411102	1847.381696	19.447232
55.573985	1872.908533	19.452250
55.647629	1878.062758	19.457267
55.731722	1882.085860	19.462285
55.680955	1883.404354	19.467303
55.731019	1885.084303	19.472320
56.010762	1897.709175	19.477338
55.740725	1907.838761	19.482355
56.082006	1894.603673	19.487373
55.610422	1892.813262	19.492391
55.889850	1887.539879	19.497408
56.158759	1887.180847	19.502426
55.903626	1893.103252	19.507443
56.462833	1885.348577	19.512461
56.189765	1887.816250	19.517479
55.830202	1884.131313	19.522496
56.464383	1888.961766	19.527514
56.616772	1896.088644	19.532531
56.733272	1884.088086	19.537549
56.490394	1880.016446	19.542567
56.437021	1885.283740	19.547584
56.777115	1882.426345	19.552602
56.447891	1895.249005	19.557619
56.830871	1903.367897	19.562637
56.913516	1908.360245	19.567655
56.982267	1912.352768	19.572672
57.364224	1913.448097	19.577690
56.967104	1899.283097	19.582707
57.090187	1873.633605	19.587725
57.104897	1877.427093	19.592743
57.468101	1873.859710	19.597760
57.321704	1881.636712	19.602778
57.157743	1882.951234	19.607795
57.150953	1883.792369	19.612813
57.063368	1890.668071	19.617831
57.264593	1899.756638	19.622848
57.670463	1906.273650	19.627866
57.214207	1913.102760	19.632883
57.429168	1908.730004	19.637901
57.354857	1904.068318	19.642919
57.481101	1911.608371	19.647936
57.495770	1905.663031	19.652954
57.444605	1907.584074	19.657971
57.596382	1902.164297	19.662989
57.657835	1915.989637	19.668007
57.896250	1928.761130	19.673024
58.111953	1928.166757	19.678042
57.977605	1937.288412	19.683059
58.180931	1940.746662	19.688077
58.454247	1936.166386	19.693095
58.273606	1935.797244	19.698112
58.373938	1927.469195	19.703130
58.286532	1931.621910	19.708147
58.385521	1931.455147	19.713165
58.160976	1932.678658	19.718183
58.134943	1935.723586	19.723200
58.401690	1926.395271	19.728218
58.167900	1934.275902	19.733235
58.696537	1936.101340	19.738253
58.384272	1928.122241	19.743271
58.260834	1940.314358	19.748288
58.643871	1950.805455	19.753306
58.570273	1957.314006	19.758323
58.963410	1959.853206	19.763341
58.876322	1959.848255	19.768359
59.213044	1960.883159	19.773376
59.284727	1945.735691	19.778394
58.958680	1961.085824	19.783411
59.237532	1949.345620	19.788429
59.460243	1945.486011	19.793447
59.531616	1955.309494	19.798464
59.159142	1958.920921	19.803482
59.132250	1951.017427	19.808499
59.730466	1941.758941	19.813517
59.836431	1948.174356	19.818535
59.838171	1948.342435	19.823552
59.876046	1942.764623	19.828570
59.723888	1948.242754	19.833587
60.062793	1934.948231	19.838605
60.093473	1935.371250	19.843623
60.014984	1948.064307	19.848640
60.338859	1942.842019	19.853658
60.192310	1950.845604	19.858675
60.504679	1938.555781	19.863693
60.262905	1938.924719	19.868711
59.943248	1924.988020	19.873728
59.970100	1926.311443	19.878746
59.986086	1957.575234	19.883763
59.948067	1938.352141	19.888781
59.774844	1936.542460	19.893799
60.186920	1933.668857	19.898816
60.217903	1942.208857	19.903834
60.175446	1952.986467	19.908851
60.428163	1966.147407	19.913869
60.785662	1962.661139	19.918887
60.501820	1967.963643	19.923904
60.703924	1965.928932	19.928922
60.583743	1964.607878	19.933939
60.480152	1971.229760	19.938957
60.941629	1960.890345	19.943975
60.763703	1968.655118	19.948992
60.951639	1963.583493	19.954010
60.637164	1982.221880	19.959027
60.887268	1985.866955	19.964045
61.132724	2005.131039	19.969063
61.228713	1997.259835	19.974080
61.492411	1987.660611	19.979098
60.993620	1993.986080	19.984115
61.135749	1995.838555	19.989133
61.350645	1981.773296	19.994151
61.517476	1998.880644	19.999168
61.644722	2011.032843	20.004186
61.441740	2015.105696	20.009203
61.935969	2013.954080	20.014221
62.242043	2011.206696	20.019239
61.755115	2020.379910	20.024256
62.038794	2011.136146	20.029274
61.953730	2014.188145	20.034291
62.343948	2015.039124	20.039309
62.348826	2006.778163	20.044327
62.108932	2009.194160	20.049344
62.208240	2010.997622	20.054362
61.983811	2010.810859	20.059379
62.393098	2002.371362	20.064397
62.338218	2001.344281	20.069415
62.212247	2003.893125	20.074432
62.391515	2005.832491	20.079450
62.787561	2007.657847	20.084467
62.207243	2003.962464	20.089485
62.476017	2006.276892	20.094503
62.713948	2011.217770	20.099520
62.976525	2026.599949	20.104538
62.886445	2038.473786	20.109555
62.881828	2024.997215	20.114573
63.155743	2025.648871	20.119591
63.182356	2035.911356	20.124608
63.123836	2030.596643	20.129626
63.029356	2029.536548	20.134643
63.066066	2031.851021	20.139661
63.145589	2035.454883	20.144679
63.254468	2025.207833	20.149696
63.379074	2026.661973	20.154714
63.491342	2029.658123	20.159731
63.336264	2029.752106	20.164749
63.525132	2022.049340	20.169767
63.403636	2028.842423	20.174784
63.635003	2019.230244	20.179802
63.763382	2018.643501	20.184819
63.775357	2020.456173	20.189837
63.937744	2013.673165	20.194855
63.793547	2020.557956	20.199872
64.081061	2043.488520	20.204890
63.830495	2042.467473	20.209907
63.920129	2044.229222	20.214925
64.159403	2032.438633	20.219943
64.050993	2036.556186	20.224960
64.243523	2040.459004	20.229978
64.313465	2047.554273	20.234995
64.379538	2049.484954	20.240013
64.511780	2036.920956	20.245031
64.519807	2034.914038	20.250048
64.434025	2057.428297	20.255066
64.387649	2055.764332	20.260083
64.503099	2053.941635	20.265101
64.920408	2061.539173	20.270119
64.732135	2071.495380	20.275136
64.960552	2072.482281	20.280154
65.041246	2073.088458	20.285171
64.986892	2077.386173	20.290189
65.100164	2073.962423	20.295207
65.344822	2073.620626	20.300224
65.370148	2078.482169	20.305242
65.067807	2073.820611	20.310259
65.045260	2063.006160	20.315277
64.911347	2082.485008	20.320295
65.204250	2069.076572	20.325312
65.505128	2086.466252	20.330330
65.630810	2099.770272	20.335347
65.372303	2094.849237	20.340365
65.811221	2097.888483	20.345383
65.596563	2089.013587	20.350400
65.548078	2097.896699	20.355418
65.702163	2100.019426	20.360435
65.509108	2101.292200	20.365453
65.907888	2097.763924	20.370471
65.641551	2113.282453	20.375488
66.242508	2112.168082	20.380506
66.385353	2120.296290	20.385523
66.329341	2120.980114	20.390541
66.390530	2111.936155	20.395559
66.505983	2115.010470	20.400576
67.057142	2113.392001	20.405594
66.944640	2099.202653	20.410611
66.630901	2094.652235	20.415629
66.943985	2078.850270	20.420647
66.576281	2070.303397	20.425664
66.699668	2077.283974	20.430682
66.900035	2079.119309	20.435699
67.016441	2093.002911	20.440717
66.829866	2090.581835	20.445735
66.653985	2111.162280	20.450752
66.947620	2111.352242	20.455770
67.056641	2113.147876	20.460787
66.800296	2118.423239	20.465805
67.368672	2117.675087	20.470823
67.023609	2109.125367	20.475840
67.309287	2110.346182	20.480858
67.310205	2111.761064	20.485875
67.456156	2136.012146	20.490893
67.676590	2131.949136	20.495911
67.429221	2137.100374	20.500928
67.634587	2127.688120	20.505946
67.816414	2131.888410	20.510963
67.901750	2137.714932	20.515981
68.174646	2137.478747	20.520999
68.062787	2135.789821	20.526016
67.888101	2125.153748	20.531034
68.211536	2137.779729	20.536051
67.927373	2132.518265	20.541069
68.256040	2129.867148	20.546087
68.169944	2136.925993	20.551104
68.261835	2129.145824	20.556122
68.261109	2140.402216	20.561139
68.140135	2153.748766	20.566157
68.310817	2154.008674	20.571175
68.405554	2151.718127	20.576192
68.701047	2168.702908	20.581210
68.775227	2159.578979	20.586227
68.607215	2160.882373	20.591245
68.740070	2163.322326	20.596263
68.704952	2164.202603	20.601280
69.022709	2173.184667	20.606298
69.301035	2185.551244	20.611315
68.915729	2197.535999	20.616333
69.375561	2190.961105	20.621351
69.055762	2184.555372	20.626368
69.313309	2185.524266	20.631386
69.583260	2183.626576	20.636403
69.546023	2190.167187	20.641421
69.572398	2187.315717	20.646439
69.296536	2185.399669	20.651456
69.395046	2187.195416	20.656474
69.518125	2190.972490	20.661491
69.230192	2191.418796	20.666509
69.981891	2200.846866	20.671527
70.025846	2201.988254	20.676544
70.187598	2217.007598	20.681562
70.481005	2205.302622	20.686579
70.405069	2206.767524	20.691597
70.654047	2196.219574	20.696615
70.135988	2183.902303	20.701632
70.191237	2175.282414	20.706650
70.274775	2181.386892	20.711667
70.317409	2209.034364	20.716685
70.717452	2203.614999	20.721703
70.767122	2207.124560	20.726720
70.460743	2192.633328	20.731738
70.562626	2202.796621	20.736755
70.765519	2197.138912	20.741773
71.245763	2192.726128	20.746791
70.921574	2201.541580	20.751808
70.796916	2192.287310	20.756826
71.128870	2190.792669	20.761843
71.147446	2192.406100	20.766861
71.284410	2193.526363	20.771879
71.103659	2192.072582	20.776896
70.856537	2195.614524	20.781914
71.299039	2203.053170	20.786931
71.400870	2216.973824	20.791949
71.368889	2222.900102	20.796967
71.492916	2231.370377	20.801984
71.569154	2236.282845	20.807002
71.661057	2221.137373	20.812019
71.753588	2229.544239	20.817037
71.397862	2219.979931	20.822055
71.993040	2228.887901	20.827072
72.082572	2235.711924	20.832090
71.989834	2243.029869	20.837107
72.119149	2237.361067	20.842125
72.679170	2233.379951	20.847143
72.500681	2238.296859	20.852160
72.423429	2236.853312	20.857178
72.552698	2228.804421	20.862195
72.459265	2237.174090	20.867213
72.538158	2230.714983	20.872231
72.790270	2233.802139	20.877248
72.490626	2232.377538	20.882266
72.760765	2236.331744	20.887283
72.800074	2237.163975	20.892301
72.884093	2229.063309	20.897319
72.955888	2232.133599	20.902336
72.501880	2237.926613	20.907354
73.178347	2251.099681	20.912371
72.911974	2269.101522	20.917389
73.012569	2268.967534	20.922407
73.209673	2265.960615	20.927424
73.080876	2269.099869	20.932442
73.412107	2271.159764	20.937459
73.229096	2269.449919	20.942477
73.606578	2274.947537	20.947495
73.745571	2302.403633	20.952512
73.586546	2298.655932	20.957530
74.132117	2285.947153	20.962547
74.092163	2292.926353	20.967565
74.125475	2300.394907	20.972583
74.366914	2286.577606	20.977600
74.581177	2280.854341	20.982618
74.471386	2263.772247	20.987635
74.359556	2255.904154	20.992653
74.050779	2243.808300	20.997671
73.952266	2267.223941	21.002688
74.069022	2285.489551	21.007706
74.239165	2281.675993	21.012723
74.231469	2283.889043	21.017741
73.994265	2279.746380	21.022759
74.459563	2294.320976	21.027776
74.590987	2307.514941	21.032794
74.581117	2328.950947	21.037811
74.527111	2322.914136	21.042829
74.727057	2315.604300	21.047847
74.876553	2318.570191	21.052864
75.058894	2329.358638	21.057882
75.591250	2334.230654	21.062899
75.433268	2343.604097	21.067917
75.459722	2329.607094	21.072935
75.729251	2339.395306	21.077952
75.392323	2334.414330	21.082970
75.660703	2330.016414	21.087987
75.854837	2335.190916	21.093005
75.644754	2332.834899	21.098023
75.870039	2334.920351	21.103040
75.611713	2329.694022	21.108058
75.883068	2330.590721	21.113075
76.025972	2331.294747	21.118093
75.816638	2338.831904	21.123111
76.070005	2338.801763	21.128128
76.091312	2349.756699	21.133146
76.360903	2343.526697	21.138163
76.468257	2362.562368	21.143181
76.548006	2346.231789	21.148199
76.656872	2343.371853	21.153216
76.304621	2351.801738	21.158234
76.665033	2357.446049	21.163251
76.368887	2351.933931	21.168269
76.441237	2352.939448	21.173287
76.821554	2370.085554	21.178304
76.702846	2379.987616	21.183322
76.885719	2375.271395	21.188339
76.872235	2386.253143	21.193357
76.969222	2375.662444	21.198375
77.369894	2374.221326	21.203392
76.816838	2385.482609	21.208410
77.259794	2389.814377	21.213427
77.635131	2393.678701	21.218445
77.430015	2404.621804	21.223463
77.848393	2397.186641	21.228480
77.994500	2402.843121	21.233498
78.157597	2392.559638	21.238515
78.138744	2416.577904	21.243533
77.954234	2407.325962	21.248551
78.327502	2391.047634	21.253568
78.047024	2399.774431	21.258586
78.229346	2390.994144	21.263603
78.253852	2405.680044	21.268621
78.380128	2396.048195	21.273639
78.374293	2392.991024	21.278656
78.120775	2402.526825	21.283674
78.215008	2401.011081	21.288691
78.375175	2400.068450	21.293709
78.106638	2411.531361	21.298727
78.317862	2422.674730	21.303744
78.607316	2426.789513	21.308762
78.775881	2432.727159	21.313779
79.045628	2427.493668	21.318797
78.478553	2428.127647	21.323815
78.911187	2438.306007	21.328832
79.158114	2449.268300	21.333850
79.653578	2442.671095	21.338867
79.481674	2440.047833	21.343885
80.003033	2445.681460	21.348903
80.271374	2435.229357	21.353920
79.836073	2435.920192	21.358938
79.806119	2413.042397	21.363955
80.136594	2396.670207	21.368973
80.271808	2409.032268	21.373991
80.120693	2409.217647	21.379008
79.639329	2403.734258	21.384026
79.950192	2403.596629	21.389043
80.184798	2419.752942	21.394061
80.344457	2426.934770	21.399079
80.847323	2423.834227	21.404096
80.337436	2440.731452	21.409114
80.593743	2441.163341	21.414131
80.741136	2433.847668	21.419149
80.438122	2449.754670	21.424167
80.343299	2430.814494	21.429184
80.223864	2429.560922	21.434202
80.486950	2433.198537	21.439219
80.597505	2437.588832	21.444237
80.453335	2450.531127	21.449255
80.761134	2458.715811	21.454272
80.800718	2465.260026	21.459290
81.045093	2460.490709	21.464307
81.430832	2454.737672	21.469325
81.312518	2462.812545	21.474343
81.467338	2457.723221	21.479360
81.701709	2468.114127	21.484378
81.750454	2477.932920	21.489395
81.790608	2468.910971	21.494413
81.780378	2467.610092	21.499431
81.922207	2473.629888	21.504448
81.807654	2484.582206	21.509466
82.039826	2490.951781	21.514483
82.150680	2478.961072	21.519501
82.021145	2485.655755	21.524519
82.060173	2485.692043	21.529536
81.849634	2491.364529	21.534554
82.082836	2480.245486	21.539571
82.468028	2479.001108	21.544589
81.943549	2491.042118	21.549607
82.592031	2496.455706	21.554624
82.430729	2504.719939	21.559642
82.531402	2509.380050	21.564659
82.783389	2509.011907	21.569677
82.676763	2515.303376	21.574695
83.095610	2504.731263	21.579712
83.044694	2516.063593	21.584730
83.141194	2523.371952	21.589747
83.442651	2531.372059	21.594765
83.428066	2532.993961	21.599783
83.641203	2522.873879	21.604800
83.493035	2532.065753	21.609818
83.637853	2534.784667	21.614835
83.854638	2527.712730	21.619853
83.875330	2528.574690	21.624871
84.044785	2530.724133	21.629888
83.951094	2529.670168	21.634906
84.056157	2524.005123	21.639923
83.915772	2516.503262	21.644941
83.956513	2516.395336	21.649959
84.358237	2517.069898	21.654976
84.385867	2518.446738	21.659994
84.306183	2519.452127	21.665011
84.465014	2527.896575	21.670029
84.284080	2527.917599	21.675047
84.466632	2524.928679	21.680064
84.593495	2549.951184	21.685082
84.877326	2555.254617	21.690099
85.135850	2544.988846	21.695117
84.786406	2552.806448	21.700135
84.937471	2541.160086	21.705152
84.733834	2555.972973	21.710170
84.963187	2555.594281	21.715187
85.245590	2564.288051	21.720205
85.315228	2577.989225	21.725223
85.377438	2574.762278	21.730240
85.475067	2573.010004	21.735258
85.431001	2571.510790	21.740275
85.788045	2571.269049	21.745293
85.783865	2581.632792	21.750311
85.943459	2577.895563	21.755328
85.994750	2566.706355	21.760346
85.701146	2565.886413	21.765363
86.124536	2563.149325	21.770381
86.175317	2568.661398	21.775399
86.214011	2558.177396	21.780416
86.325789	2575.425561	21.785434
86.342356	2591.115003	21.790451
86.642522	2587.603912	21.795469
86.878128	2588.784775	21.800487
87.147703	2572.808305	21.805504
87.005892	2579.716575	21.810522
86.868657	2589.493523	21.815539
86.851311	2581.818627	21.820557
86.908482	2582.552069	21.825575
86.909710	2576.143736	21.830592
87.420497	2579.459512	21.835610
87.056400	2587.413972	21.840627
87.442141	2576.783376	21.845645
86.990927	2575.814734	21.850663
87.518033	2580.137861	21.855680
87.404314	2580.017596	21.860698
87.392811	2608.829144	21.865715
87.524321	2609.660066	21.870733
87.470390	2615.755972	21.875751
87.803555	2607.589410	21.880768
87.800761	2603.598050	21.885786
87.720986	2609.639081	21.890803
88.012238	2622.089707	21.895821
88.036150	2630.326837	21.900839
88.289005	2638.462965	21.905856
88.620039	2633.528752	21.910874
88.131246	2629.448129	21.915891
88.526337	2631.615095	21.920909
88.853819	2633.287863	21.925927
89.171868	2627.198677	21.930944
88.944312	2628.001907	21.935962
88.707006	2647.254945	21.940979
89.165864	2647.160575	21.945997
89.242222	2659.261654	21.951015
89.608673	2661.937384	21.956032
89.638246	2656.696490	21.961050
89.186320	2662.923524	21.966067
89.729837	2654.648669	21.971085
89.538881	2657.590262	21.976103
89.702524	2648.951235	21.981120
89.472578	2657.050308	21.986138
89.568350	2653.213904	21.991155
89.807425	2651.598741	21.996173
89.503890	2659.685165	22.001191
90.052094	2668.820356	22.006208
90.213683	2669.421526	22.011226
90.000747	2677.479355	22.016243
90.061456	2676.528970	22.021261
90.542663	2671.990042	22.026279
90.432959	2668.232806	22.031296
90.518670	2663.711325	22.036314
90.441183	2665.058533	22.041331
90.726615	2660.602740	22.046349
90.475511	2676.250007	22.051367
90.796318	2689.269391	22.056384
91.051560	2691.346186	22.061402
91.255344	2694.187872	22.066419
91.485607	2689.998078	22.071437
91.370645	2694.206530	22.076455
91.454731	2698.274696	22.081472
91.323309	2691.885105	22.086490
91.282073	2697.124800	22.091507
91.549872	2694.880511	22.096525
91.215323	2694.809616	22.101543
91.363038	2706.631920	22.106560
91.848368	2716.684876	22.111578
92.148122	2717.493696	22.116595
92.021582	2711.058483	22.121613
92.180360	2714.697072	22.126631
92.116747	2721.979935	22.131648
92.119529	2715.667256	22.136666
91.901126	2709.947531	22.141683
92.560685	2725.612459	22.146701
92.512944	2743.156841	22.151719
92.747017	2740.550592	22.156736
92.791056	2747.703822	22.161754
92.802439	2744.290657	22.166771
92.879723	2736.610029	22.171789
92.798048	2740.622835	22.176807
93.163286	2745.151951	22.181824
93.574576	2755.884545	22.186842
93.321510	2765.917627	22.191859
93.622286	2757.830872	22.196877
93.642758	2762.704431	22.201895
93.641116	2767.996044	22.206912
93.693834	2755.874367	22.211930
93.665946	2755.591750	22.216947
93.790405	2759.764403	22.221965
93.916238	2759.403787	22.226983
94.167768	2759.760938	22.232000
94.347284	2755.266159	22.237018
93.952730	2756.643483	22.242035
94.185314	2763.648669	22.247053
94.317767	2780.218895	22.252071
94.204187	2787.230523	22.257088
94.611385	2783.334987	22.262106
94.751034	2792.677775	22.267123
94.857306	2770.488764	22.272141
95.285382	2783.980381	22.277159
94.803975	2790.728952	22.282176
95.101151	2777.072989	22.287194
95.054393	2780.873368	22.292211
95.141841	2776.176954	22.297229
95.381938	2808.564682	22.302247
95.578868	2819.352742	22.307264
95.585342	2818.475495	22.312282
95.816083	2806.219988	22.317299
95.575788	2818.955335	22.322317
95.543675	2822.623603	22.327335
95.560140	2824.990199	22.332352
95.701007	2819.010205	22.337370
95.491728	2817.838571	22.342387
95.862800	2820.892727	22.347405
95.942056	2838.412254	22.352423
96.042452	2841.057292	22.357440
96.267739	2841.969238	22.362458
96.126283	2856.902301	22.367475
96.733582	2829.234987	22.372493
96.491917	2851.396196	22.377511
96.777209	2859.427380	22.382528
97.134716	2863.433903	22.387546
96.875239	2881.944316	22.392563
97.195688	2855.091187	22.397581
97.242667	2860.243722	22.402599
97.246800	2867.816330	22.407616
97.466201	2867.844309	22.412634
97.305748	2864.991821	22.417651
97.489037	2865.815288	22.422669
97.411865	2860.550440	22.427687
97.512478	2884.927989	22.432704
97.923988	2880.640807	22.437722
97.939535	2896.654814	22.442739
98.054984	2893.651350	22.447757
98.516504	2884.673650	22.452775
98.190827	2887.063349	22.457792
98.185240	2875.049980	22.462810
98.246080	2878.808843	22.467827
98.361590	2875.713343	22.472845
98.521938	2889.239883	22.477863
98.488721	2908.060349	22.482880
98.728769	2907.446328	22.487898
98.776582	2922.365010	22.492915
98.679543	2921.464933	22.497933
98.887364	2909.631458	22.502951
98.570464	2910.976748	22.507968
99.115553	2915.086308	22.512986
99.095879	2924.416043	22.518003
99.615547	2933.957113	22.523021
99.343102	2936.570376	22.528039
99.246032	2934.491208	22.533056
99.711655	2941.361784	22.538074
99.969778	2961.158427	22.543091
100.095751	2958.143833	22.548109
100.267562	2965.334216	22.553127
100.330595	2952.291209	22.558144
100.303033	2955.191074	22.563162
100.297932	2955.921093	22.568179
100.520421	2952.504108	22.573197
100.633701	2966.271842	22.578215
100.427684	2961.369668	22.583232
100.798035	2944.704977	22.588250
100.723179	2951.859960	22.593267
101.172623	2956.289979	22.598285
101.194501	2950.456332	22.603303
101.186488	2940.893520	22.608320
101.181339	2939.244903	22.613338
101.245638	2950.019599	22.618355
101.098059	2949.712801	22.623373
101.270184	2961.332414	22.628391
101.502455	2971.283527	22.633408
101.725407	2974.521013	22.638426
101.819568	2990.296050	22.643443
101.515520	2986.863905	22.648461
101.839127	2984.655511	22.653479
101.693030	2978.424665	22.658496
101.660253	3001.479396	22.663514
101.498295	3009.477364	22.668531
102.090449	2998.668030	22.673549
102.588620	3008.934669	22.678567
102.314935	3031.800537	22.683584
102.878020	3029.501249	22.688602
102.752659	3029.840632	22.693619
102.713253	3032.301909	22.698637
103.022311	3030.082456	22.703655
103.048837	3030.687873	22.708672
103.082371	3025.576003	22.713690
103.099492	3023.274100	22.718707
103.363802	3027.580276	22.723725
103.159577	3037.114921	22.728743
103.258218	3052.230932	22.733760
103.643760	3046.877289	22.738778
103.590866	3048.939557	22.743795
103.771573	3048.786498	22.748813
104.307070	3044.178235	22.753831
104.281440	3056.402882	22.758848
104.470206	3063.649606	22.763866
104.407991	3077.384074	22.768883
105.007328	3047.132867	22.773901
104.621767	3042.189288	22.778919
104.356452	3046.238539	22.783936
104.745405	3046.749983	22.788954
104.795332	3048.666068	22.793971
104.733907	3071.007317	22.798989
105.148290	3062.402792	22.804007
104.692768	3061.740784	22.809024
104.859339	3054.821335	22.814042
104.857357	3065.531959	22.819059
105.161792	3077.678037	22.824077
105.413426	3099.969412	22.829095
105.333135	3098.198251	22.834112
105.531238	3091.299714	22.839130
105.672319	3100.942952	22.844147
105.609583	3108.112597	22.849165
105.859227	3123.617568	22.854183
106.086099	3095.189992	22.859200
106.200135	3110.270572	22.864218
106.370804	3119.205100	22.869235
106.650368	3108.987496	22.874253
106.960232	3110.461763	22.879271
106.350298	3119.472778	22.884288
106.661116	3118.276395	22.889306
106.604951	3108.136709	22.894323
106.628893	3129.814707	22.899341
107.111277	3137.067351	22.904359
107.259264	3137.474847	22.909376
107.384614	3139.091023	22.914394
107.480892	3149.216543	22.919411
107.528590	3134.901527	22.924429
107.732053	3134.593812	22.929447
107.719288	3138.356613	22.934464
107.695917	3120.197037	22.939482
107.873170	3121.609072	22.944499
107.679472	3129.889835	22.949517
108.129089	3127.967314	22.954535
108.194964	3131.457996	22.959552
108.174792	3153.797513	22.964570
108.482430	3161.100845	22.969587
108.679616	3151.923646	22.974605
108.851285	3155.670415	22.979623
108.783228	3157.418116	22.984640
108.985449	3151.642159	22.989658
108.715361	3160.458995	22.994675
109.117841	3153.976202	22.999693
109.286710	3148.485593	23.004711
108.846142	3154.558420	23.009728
109.323213	3161.292768	23.014746
109.430017	3179.982708	23.019763
109.458024	3163.638227	23.024781
109.754319	3190.585585	23.029799
109.722382	3175.599671	23.034816
109.807180	3170.029641	23.039834
109.977742	3180.358867	23.044851
109.541226	3177.835870	23.049869
109.580421	3183.760629	23.054887
109.979682	3198.090239	23.059904
110.151687	3217.263815	23.064922
110.147154	3215.906899	23.069939
110.466267	3225.442385	23.074957
111.102660	3223.651325	23.079975
110.989280	3231.564581	23.084992
111.214651	3232.388440	23.090010
111.404999	3229.899990	23.095027
111.107139	3228.086417	23.100045
111.232906	3213.144539	23.105063
111.419512	3220.002317	23.110080
111.484663	3230.721236	23.115098
111.598165	3218.429803	23.120115
111.164159	3230.481372	23.125133
111.953328	3233.757637	23.130151
111.735228	3245.910875	23.135168
111.742971	3252.916752	23.140186
112.040233	3252.669593	23.145203
112.189296	3260.034443	23.150221
112.123573	3253.342298	23.155239
112.080346	3265.264724	23.160256
112.498254	3277.092393	23.165274
112.615736	3267.352035	23.170291
112.726307	3286.466277	23.175309
112.973509	3275.053356	23.180327
112.971684	3278.171791	23.185344
112.847346	3269.594051	23.190362
112.930465	3286.180586	23.195379
113.065868	3294.634722	23.200397
113.516494	3292.437495	23.205415
113.322674	3304.568031	23.210432
113.593593	3300.117508	23.215450
113.895771	3310.811278	23.220467
113.684607	3306.322777	23.225485
114.095117	3292.598708	23.230503
113.969615	3298.039266	23.235520
114.300008	3307.655603	23.240538
114.747154	3315.639209	23.245555
114.504857	3326.453631	23.250573
114.361341	3324.870297	23.255591
114.678698	3322.374165	23.260608
114.794130	3309.612743	23.265626
114.907617	3329.215060	23.270643
114.778175	3317.337494	23.275661
115.149415	3303.061971	23.280679
114.973875	3323.035234	23.285696
115.076722	3344.050443	23.290714
115.316455	3347.636953	23.295731
115.179087	3355.120678	23.300749
115.448249	3354.564141	23.305767
115.432164	3360.904464	23.310784
115.570986	3377.664715	23.315802
116.050547	3375.763348	23.320819
115.842114	3381.837797	23.325837
115.944988	3377.075803	23.330855
116.170491	3389.968637	23.335872
116.553814	3400.289266	23.340890
116.782300	3403.762738	23.345907
116.712917	3402.610438	23.350925
117.040822	3404.977026	23.355943
116.948521	3414.037834	23.360960
116.855912	3403.954096	23.365978
117.134179	3398.186369	23.370995
117.190987	3409.293764	23.376013
117.058569	3409.274011	23.381031
117.067166	3411.311579	23.386048
117.385894	3425.132729	23.391066
117.918060	3413.398950	23.396083
117.626038	3421.102447	23.401101
117.891150	3415.657750	23.406119
117.842683	3420.810756	23.411136
118.027272	3431.964655	23.416154
118.462466	3432.339739	23.421171
118.387424	3443.437504	23.426189
118.436816	3443.720713	23.431207
118.408352	3443.078691	23.436224
118.081522	3447.141005	23.441242
118.260477	3445.996302	23.446259
118.448692	3471.268617	23.451277
118.765678	3457.092844	23.456295
118.490010	3464.527880	23.461312
119.120125	3472.309344	23.466330
119.298995	3500.712361	23.471347
119.278789	3503.490810	23.476365
119.763818	3489.647696	23.481383
120.163500	3492.359192	23.486400
120.107760	3487.692462	23.491418
120.140605	3486.083349	23.496435
120.097386	3488.185827	23.501453
120.212474	3483.308578	23.506471
120.375543	3493.979826	23.511488
120.376606	3509.884329	23.516506
120.732138	3509.627877	23.521523
120.697008	3511.730641	23.526541
120.686392	3519.589908	23.531559
121.017569	3501.079919	23.536576
120.992483	3501.446587	23.541594
120.907469	3520.298912	23.546611
120.989436	3525.157414	23.551629
121.088110	3523.087067	23.556647
121.357613	3530.612987	23.561664
121.672676	3535.295095	23.566682
121.902560	3520.728826	23.571699
121.781708	3539.948735	23.576717
121.982084	3544.352576	23.581735
122.325776	3563.267180	23.586752
122.359516	3560.303354	23.591770
122.575346	3554.775215	23.596787
122.632126	3559.800575	23.601805
122.567097	3550.823048	23.606823
122.616032	3556.703928	23.611840
122.600147	3566.416553	23.616858
123.042471	3540.077641	23.621875
122.984887	3603.166866	23.626893
123.198308	3589.033438	23.631911
123.215910	3578.651969	23.636928
123.005796	3594.611474	23.641946
123.624936	3581.057607	23.646963
123.699078	3594.098256	23.651981
123.815456	3593.399309	23.656999
123.699478	3602.781017	23.662016
123.675046	3615.639173	23.667034
123.980427	3601.906407	23.672051
123.936909	3615.491301	23.677069
124.410051	3629.490188	23.682087
124.358705	3639.000846	23.687104
124.524682	3635.469216	23.692122
124.804061	3639.073077	23.697139
124.388593	3638.904944	23.702157
124.870357	3649.648993	23.707175
124.697825	3641.755215	23.712192
124.747615	3668.406086	23.717210
125.088970	3668.810299	23.722227
124.698001	3679.323808	23.727245
125.178863	3682.856223	23.732263
125.554127	3687.043432	23.737280
125.481470	3711.682043	23.742298
125.727102	3702.682422	23.747315
126.031829	3708.333787	23.752333
126.208455	3718.088975	23.757351
126.424005	3724.027526	23.762368
126.443129	3726.049300	23.767386
126.718517	3725.899233	23.772403
126.860325	3733.252895	23.777421
126.779660	3724.672642	23.782439
126.932073	3729.440530	23.787456
126.934829	3714.586192	23.792474
127.033908	3730.296741	23.797491
126.952498	3763.294001	23.802509
127.289733	3750.338717	23.807527
127.330388	3752.832188	23.812544
127.515113	3755.223238	23.817562
127.816055	3765.388923	23.822579
128.168862	3774.194911	23.827597
128.105327	3776.432037	23.832615
128.267782	3763.535288	23.837632
128.062766	3761.953058	23.842650
128.274226	3761.835209	23.847667
128.474287	3782.665636	23.852685
128.866122	3783.824053	23.857703
129.267463	3788.966827	23.862720
128.615945	3798.312120	23.867738
129.127931	3789.030840	23.872755
129.169414	3781.691266	23.877773
129.367343	3789.818708	23.882791
129.639650	3782.089918	23.887808
129.507820	3793.418833	23.892826
129.625007	3802.533795	23.897843
129.753176	3823.201110	23.902861
129.942853	3811.965286	23.907879
130.243561	3812.688279	23.912896
129.730418	3810.940421	23.917914
130.067697	3805.284269	23.922931
130.216006	3826.082104	23.927949
130.254303	3841.957432	23.932967
130.462645	3839.213501	23.937984
130.387502	3844.327644	23.943002
130.553909	3860.995162	23.948019
130.721674	3871.927102	23.953037
131.092300	3877.037832	23.958055
131.077552	3877.673465	23.963072
130.908299	3896.669500	23.968090
131.543720	3897.730877	23.973107
131.654251	3896.095174	23.978125
131.826749	3908.439978	23.983143
131.851143	3897.574990	23.988160
132.118140	3921.189086	23.993178
132.119875	3918.914668	23.998195
132.376815	3925.896868	24.003213
132.666426	3921.377889	24.008231
133.214908	3920.564406	24.013248
132.778794	3930.797380	24.018266
132.624649	3920.771869	24.023283
132.806443	3916.582378	24.028301
132.753788	3924.394287	24.033319
133.355967	3937.835622	24.038336
133.505332	3939.878352	24.043354
133.534798	3945.845090	24.048371
133.547225	3942.080638	24.053389
133.495489	3943.596130	24.058407
134.034601	3950.857448	24.063424
133.870863	3976.201699	24.068442
133.998177	3962.623638	24.073459
134.340389	3966.671457	24.078477
134.327656	3963.026647	24.083495
134.261361	3963.311793	24.088512
134.730872	3987.774748	24.093530
134.711774	3996.226393	24.098547
134.793693	3991.365278	24.103565
135.080134	4007.592182	24.108583
134.974005	3998.359767	24.113600
134.819627	4016.876092	24.118618
135.355315	4014.623510	24.123635
135.634534	4014.827608	24.128653
135.772802	4028.785089	24.133671
135.951002	4028.820433	24.138688
136.342212	4035.863089	24.143706
136.453725	4041.327490	24.148723
136.778723	4045.723414	24.153741
136.824048	4049.726553	24.158759
137.460079	4041.326838	24.163776
136.818776	4037.583993	24.168794
137.018666	4041.534955	24.173811
136.977169	4044.696851	24.178829
136.864781	4044.944508	24.183847
136.797400	4041.969175	24.188864
137.168282	4039.362916	24.193882
137.251117	4038.019525	24.198899
137.454338	4074.925007	24.203917
137.698033	4065.215916	24.208935
137.899830	4062.601212	24.213952
137.665605	4063.572346	24.218970
138.226329	4090.825333	24.223987
138.095804	4089.130497	24.229005
138.450137	4084.636549	24.234023
138.485401	4097.755431	24.239040
138.305657	4098.311182	24.244058
138.676980	4103.624052	24.249075
138.891308	4117.574211	24.254093
139.015060	4126.563251	24.259111
139.248626	4119.946494	24.264128
138.963523	4126.903509	24.269146
139.092648	4127.749849	24.274163
139.675504	4145.996970	24.279181
139.779643	4160.185787	24.284199
139.806322	4147.086154	24.289216
139.962517	4155.955188	24.294234
140.007633	4150.469779	24.299251
140.329535	4166.925630	24.304269
140.286837	4171.907276	24.309287
140.371371	4176.573642	24.314304
140.516253	4179.291284	24.319322
140.747844	4184.253587	24.324339
141.246152	4188.413459	24.329357
141.007503	4209.562238	24.334375
141.397356	4206.425865	24.339392
141.314808	4210.490343	24.344410
141.727973	4206.359854	24.349427
141.645278	4199.613342	24.354445
141.494005	4228.125475	24.359463
141.788146	4221.676800	24.364480
141.543626	4219.847513	24.369498
141.683965	4222.095467	24.374515
142.174611	4236.644383	24.379533
142.568567	4246.911214	24.384551
142.375926	4252.287309	24.389568
142.430773	4256.578478	24.394586
142.927702	4266.514242	24.399603
143.233066	4268.810625	24.404621
143.091040	4278.404595	24.409639
143.640197	4266.828699	24.414656
143.751871	4262.251454	24.419674
143.708883	4267.669774	24.424691
143.667960	4285.896165	24.429709
143.674887	4296.594469	24.434727
144.198392	4304.275385	24.439744
144.315481	4306.203741	24.444762
144.248403	4303.989795	24.449779
144.684049	4312.395079	24.454797
144.529915	4318.266162	24.459815
144.809085	4328.382220	24.464832
144.806849	4323.543066	24.469850
144.742686	4325.491669	24.474867
145.241617	4333.634357	24.479885
145.467679	4345.760952	24.484903
145.357004	4345.854155	24.489920
145.296177	4352.555251	24.494938
145.404009	4356.253511	24.499955
145.754937	4363.076976	24.504973
145.729750	4384.431118	24.509991
146.228278	4377.252017	24.515008
146.379251	4371.978568	24.520026
146.059239	4372.959464	24.525043
146.313483	4381.617123	24.530061
146.506574	4395.890320	24.535079
146.872963	4395.230142	24.540096
146.927459	4400.056342	24.545114
147.227751	4399.018089	24.550131
147.847593	4405.417167	24.555149
147.546373	4409.793471	24.560167
148.051667	4411.989561	24.565184
148.132781	4408.359570	24.570202
148.401533	4435.499272	24.575219
148.528789	4401.187400	24.580237
148.552447	4413.509162	24.585255
148.981185	4425.047336	24.590272
148.798354	4421.674971	24.595290
148.721939	4413.988078	24.600307
148.599839	4403.190912	24.605325
148.698276	4430.934386	24.610343
148.915146	4412.863918	24.615360
149.053826	4422.541454	24.620378
148.829746	4455.922524	24.625395
149.117374	4448.334119	24.630413
149.052025	4447.174798	24.635431
149.596291	4473.695590	24.640448
149.711003	4480.460011	24.645466
149.906698	4477.311272	24.650483
149.928472	4482.679226	24.655501
150.266978	4498.534934	24.660519
150.745479	4499.660716	24.665536
150.816911	4497.216976	24.670554
150.756915	4495.300806	24.675571
151.114651	4500.413815	24.680589
151.291756	4520.530722	24.685607
151.324476	4522.799814	24.690624
151.232556	4523.892248	24.695642
151.563780	4527.493574	24.700659
151.901949	4505.861263	24.705677
151.704770	4527.900694	24.710695
151.916823	4542.880590	24.715712
152.441063	4539.691257	24.720730
152.388365	4538.975169	24.725747
152.497403	4551.887600	24.730765
152.635314	4548.025892	24.735783
152.660058	4548.894406	24.740800
153.022214	4575.516004	24.745818
152.925404	4575.433141	24.750835
153.310338	4558.962545	24.755853
153.236946	4573.663086	24.760871
153.355382	4604.214492	24.765888
153.594463	4600.314613	24.770906
153.559059	4613.853509	24.775923
153.909704	4600.298255	24.780941
153.628678	4623.095392	24.785959
154.126069	4631.172412	24.790976
154.538497	4625.767507	24.795994
154.479721	4631.808381	24.801011
155.014859	4621.929738	24.806029
154.826372	4623.436421	24.811047
154.709202	4644.391027	24.816064
155.218007	4642.536768	24.821082
155.208226	4642.998573	24.826099
154.996696	4643.863855	24.831117
155.236710	4666.753418	24.836135
155.708085	4662.765354	24.841152
155.913276	4667.310371	24.846170
155.620660	4683.143393	24.851187
156.168244	4681.386789	24.856205
156.366964	4689.607435	24.861223
156.330908	4696.776749	24.866240
156.743188	4695.284014	24.871258
156.528673	4712.928931	24.876275
157.219188	4706.718938	24.881293
157.515389	4725.402683	24.886311
157.465152	4708.693707	24.891328
157.781754	4733.249158	24.896346
157.673314	4733.617346	24.901363
158.149737	4706.055489	24.906381
157.919824	4737.218107	24.911399
158.154021	4723.567237	24.916416
158.414668	4726.238205	24.921434
158.465814	4737.374257	24.926451
158.798009	4748.114648	24.931469
158.794815	4753.308103	24.936487
158.648575	4752.098720	24.941504
158.746218	4750.407550	24.946522
158.733203	4760.673548	24.951539
159.158892	4771.978838	24.956557
159.232084	4780.363512	24.961575
159.005538	4784.353556	24.966592
159.605573	4795.101627	24.971610
159.433171	4818.817120	24.976627
159.930780	4826.596847	24.981645
159.963581	4829.973632	24.986663
160.251554	4829.255925	24.991680
160.743183	4841.196628	24.996698
160.809598	4870.885229	25.001715
160.933382	4854.110583	25.006733
160.941813	4864.986066	25.011751
160.663831	4872.116153	25.016768
161.181365	4890.174801	25.021786
161.471035	4884.437723	25.026803
162.099190	4883.248045	25.031821
162.041291	4913.702336	25.036839
162.044591	4889.440227	25.041856
162.232831	4886.579733	25.046874
162.353225	4926.438859	25.051891
162.684491	4909.177148	25.056909
163.040942	4919.965720	25.061927
162.750209	4904.721140	25.066944
163.008151	4932.348875	25.071962
163.234047	4903.088784	25.076979
163.251863	4912.004726	25.081997
163.390181	4919.804024	25.087015
163.580667	4913.544648	25.092032
164.027164	4957.104397	25.097050
163.336502	4943.345884	25.102067
163.885874	4924.217957	25.107085
163.894821	4953.929262	25.112103
164.034014	4986.150669	25.117120
164.621192	4957.562926	25.122138
164.571762	4980.088469	25.127155
164.862830	4990.635774	25.132173
164.984689	4990.270236	25.137191
164.897074	4997.086034	25.142208
165.349846	4990.684113	25.147226
165.270194	4997.695317	25.152243
165.688268	5020.572779	25.157261
166.112313	5016.013944	25.162279
166.004083	5017.278941	25.167296
166.149086	5023.536871	25.172314
166.255321	5026.002796	25.177331
166.343989	5025.658283	25.182349
166.258926	5046.996972	25.187367
166.746361	5035.901554	25.192384
167.149097	5045.241605	25.197402
167.058979	5057.073836	25.202419
167.139004	5071.051823	25.207437
167.495077	5060.361241	25.212455
167.464790	5052.656431	25.217472
167.834223	5070.769597	25.222490
167.931114	5086.169627	25.227507
168.366134	5087.061662	25.232525
168.330156	5079.396294	25.237543
167.947652	5102.636742	25.242560
168.611555	5103.734593	25.247578
168.598664	5116.263380	25.252595
168.755059	5133.466541	25.257613
168.959567	5124.364834	25.262631
168.942937	5132.749869	25.267648
169.164540	5151.697009	25.272666
169.206531	5155.866978	25.277683
169.878402	5171.876387	25.282701
169.641345	5184.407928	25.287719
169.878022	5178.066340	25.292736
170.475563	5185.313461	25.297754
170.356392	5209.280708	25.302771
170.652195	5204.091653	25.307789
171.118895	5193.784560	25.312807
170.983844	5222.192973	25.317824
171.624791	5227.443605	25.322842
171.972990	5242.190100	25.327859
171.776067	5227.012833	25.332877
171.648736	5231.463138	25.337895
171.648567	5234.525082	25.342912
171.864342	5226.751844	25.347930
171.802495	5231.302636	25.352947
171.935321	5231.497056	25.357965
172.347437	5260.982643	25.362983
172.278174	5257.151419	25.368000
172.417467	5262.262548	25.373018
172.883808	5274.578967	25.378035
173.013968	5278.814373	25.383053
173.220817	5277.211153	25.388071
173.002579	5302.910168	25.393088
173.678338	5302.024412	25.398106
173.634110	5312.986506	25.403123
173.727000	5322.192826	25.408141
173.918665	5323.978048	25.413159
173.816112	5342.383142	25.418176
174.119830	5346.057503	25.423194
174.510551	5363.829349	25.428211
174.754154	5367.850802	25.433229
174.689794	5362.719897	25.438247
174.983586	5386.342311	25.443264
175.366908	5377.315788	25.448282
175.355632	5394.754466	25.453299
175.416623	5404.473358	25.458317
176.360049	5403.926484	25.463335
176.155196	5414.242402	25.468352
176.296880	5408.380025	25.473370
176.533127	5414.969733	25.478387
176.729203	5419.887772	25.483405
177.009649	5428.177623	25.488423
177.050116	5446.922725	25.493440
177.491105	5446.175878	25.498458
177.329614	5441.065151	25.503475
177.661172	5446.715280	25.508493
177.998920	5435.630055	25.513511
177.739038	5460.649962	25.518528
178.164745	5449.953506	25.523546
178.092588	5462.765028	25.528563
177.999843	5462.624867	25.533581
178.018253	5471.872264	25.538599
178.353023	5489.826261	25.543616
178.324276	5485.912206	25.548634
178.996872	5510.708014	25.553651
178.941282	5530.298532	25.558669
179.216189	5516.333618	25.563687
179.177449	5531.240431	25.568704
179.571424	5542.877866	25.573722
179.846207	5564.663441	25.578739
180.125553	5558.690946	25.583757
180.468347	5568.173845	25.588775
180.119686	5584.229966	25.593792
180.598177	5572.048317	25.598810
180.713483	5579.182127	25.603827
181.211153	5600.485360	25.608845
181.464898	5597.744099	25.613863
181.319036	5599.600472	25.618880
181.385479	5602.289189	25.623898
181.650228	5597.591936	25.628915
181.854015	5599.422463	25.633933
182.084889	5614.168368	25.638951
182.129937	5628.428602	25.643968
182.415950	5623.397523	25.648986
182.607502	5610.658949	25.654003
182.716502	5627.348641	25.659021
182.892170	5627.641660	25.664039
182.906840	5657.272437	25.669056
183.341210	5658.000975	25.674074
183.451103	5653.718610	25.679092
183.478087	5670.822661	25.684109
184.135095	5671.452767	25.689127
183.563126	5671.444073	25.694144
184.304094	5669.943692	25.699162
184.586135	5685.653916	25.704180
184.374528	5697.598862	25.709197
185.021284	5708.863343	25.714215
184.648968	5700.654138	25.719232
184.925767	5701.008923	25.724250
185.040604	5726.026185	25.729268
185.475326	5731.137585	25.734285
185.512722	5721.430403	25.739303
185.503179	5744.827966	25.744320
185.759934	5753.482105	25.749338
185.855903	5761.715801	25.754356
186.192176	5779.876826	25.759373
186.366674	5791.759509	25.764391
186.593751	5806.138804	25.769408
186.907081	5801.428234	25.774426
187.070437	5814.251294	25.779444
187.188858	5817.901817	25.784461
187.446680	5812.680057	25.789479
187.572212	5831.308236	25.794496
188.035355	5838.744689	25.799514
188.053343	5858.445071	25.804532
188.605476	5850.003439	25.809549
188.722097	5842.893177	25.814567
188.849048	5866.730992	25.819584
189.084148	5868.963308	25.824602
189.057617	5876.403890	25.829620
189.105802	5872.425543	25.834637
189.433564	5870.383650	25.839655
189.360962	5881.408122	25.844672
189.295087	5884.691523	25.849690
189.762629	5887.926078	25.854708
189.771504	5907.944250	25.859725
189.876699	5915.694285	25.864743
190.074393	5934.134860	25.869760
190.450365	5942.442818	25.874778
190.546138	5958.337230	25.879796
190.511435	5960.991786	25.884813
191.313182	5971.703066	25.889831
191.324302	5990.772171	25.894848
191.468592	5993.250289	25.899866
191.718883	5985.961299	25.904884
191.736028	6000.807751	25.909901
192.110747	6011.022248	25.914919
192.233595	6012.876745	25.919936
192.378401	6012.121232	25.924954
192.360844	6021.908125	25.929972
192.560988	6040.320905	25.934989
192.894011	6051.170694	25.940007
193.073604	6052.894990	25.945024
193.294564	6054.486812	25.950042
193.607839	6056.015924	25.955060
193.570341	6072.714526	25.960077
194.035054	6092.521024	25.965095
194.084214	6107.917143	25.970112
194.493912	6095.802681	25.975130
194.779310	6096.650190	25.980148
194.804856	6123.295998	25.985165
194.974958	6127.141344	25.990183
195.193810	6128.254374	25.995200
195.096560	6126.336061	26.000218
195.319978	6145.059179	26.005236
195.455641	6170.425555	26.010253
195.969695	6149.823361	26.015271
195.802733	6179.945968	26.020288
196.010756	6196.241298	26.025306
196.284901	6189.615581	26.030324
196.392595	6207.077950	26.035341
197.055216	6209.115498	26.040359
197.076269	6233.984924	26.045376
197.016581	6251.191580	26.050394
197.415758	6247.673297	26.055412
197.682658	6245.897544	26.060429
197.859471	6249.391741	26.065447
197.971015	6278.193231	26.070464
198.062689	6281.911862	26.075482
198.428623	6293.201106	26.080500
198.523194	6287.625196	26.085517
198.722035	6300.669611	26.090535
199.105132	6326.428746	26.095552
199.235852	6333.536075	26.100570
199.500104	6323.514605	26.105588
199.619927	6338.548801	26.110605
199.797684	6349.200906	26.115623
199.846273	6351.974431	26.120640
200.374942	6350.953147	26.125658
200.961293	6369.239469	26.130676
200.582283	6368.648479	26.135693
201.032487	6388.401828	26.140711
201.017266	6360.307099	26.145728
201.196523	6393.219125	26.150746
201.743297	6388.077772	26.155764
201.878855	6398.897142	26.160781
201.983930	6408.071514	26.165799
201.949791	6385.336895	26.170816
201.928580	6411.697211	26.175834
202.324443	6421.808704	26.180852
202.489975	6422.780769	26.185869
202.432810	6463.143629	26.190887
202.699020	6426.861563	26.195904
203.003196	6466.740399	26.200922
202.990911	6452.593797	26.205940
203.675940	6480.826687	26.210957
203.688108	6473.783128	26.215975
203.525279	6485.365308	26.220992
203.771124	6508.152165	26.226010
204.293120	6500.094202	26.231028
204.154802	6517.464763	26.236045
204.470991	6526.883288	26.241063
204.962228	6550.717635	26.246080
205.273140	6548.510756	26.251098
205.616651	6552.104337	26.256116
205.509998	6564.421919	26.261133
205.722528	6582.499018	26.266151
206.092152	6567.380331	26.271168
205.988404	6583.881573	26.276186
206.844820	6592.858397	26.281204
206.703924	6603.090985	26.286221
206.851390	6581.157960	26.291239
206.847143	6607.572568	26.296256
207.336278	6630.925081	26.301274
207.362470	6621.031054	26.306292
207.607963	6623.511243	26.311309
207.674456	6650.676258	26.316327
207.943366	6650.792359	26.321344
208.245182	6642.754470	26.326362
208.655913	6672.070798	26.331380
208.506076	6677.449598	26.336397
208.917285	6690.097794	26.341415
209.328972	6681.173755	26.346432
209.076795	6707.920749	26.351450
209.464524	6718.125798	26.356468
209.640246	6720.844507	26.361485
209.738896	6737.309721	26.366503
210.200018	6745.477102	26.371520
210.201916	6746.636567	26.376538
210.827546	6758.218371	26.381556
210.986395	6771.787287	26.386573
211.198549	6783.088047	26.391591
211.249615	6785.795955	26.396608
211.528684	6788.929366	26.401626
211.705787	6793.240339	26.406644
211.884004	6800.769125	26.411661
211.869104	6783.222886	26.416679
212.187411	6806.632808	26.421696
211.981537	6817.185112	26.426714
212.503620	6826.218524	26.431732
212.577684	6846.822391	26.436749
212.873870	6847.330692	26.441767
213.129103	6848.562294	26.446784
213.390473	6885.877831	26.451802
213.815610	6877.448002	26.456820
213.650142	6879.517732	26.461837
213.970819	6878.492594	26.466855
214.296583	6900.424655	26.471872
214.239695	6907.245873	26.476890
214.656288	6899.498763	26.481908
214.824386	6923.592152	26.486925
214.817060	6928.913706	26.491943
215.104892	6928.595627	26.496960
215.275543	6952.500611	26.501978
215.453579	6956.632093	26.506996
215.705236	6971.874877	26.512013
216.036029	6973.930030	26.517031
216.793926	6992.445494	26.522048
216.497886	7000.998082	26.527066
216.930482	6997.225669	26.532084
217.113261	7011.346475	26.537101
217.226701	7011.547161	26.542119
217.789231	7010.846966	26.547136
217.826161	7030.069082	26.552154
217.841769	7037.439797	26.557172
217.690260	7041.657667	26.562189
218.003031	7055.079565	26.567207
218.591980	7072.005957	26.572224
218.359189	7081.621716	26.577242
218.963819	7095.644670	26.582260
219.115856	7103.605022	26.587277
219.315159	7109.866200	26.592295
219.386109	7126.609285	26.597312
219.633981	7131.654188	26.602330
220.075555	7131.467388	26.607348
219.975132	7158.862939	26.612365
220.519320	7168.798661	26.617383
220.994666	7172.645980	26.622400
220.606054	7193.873278	26.627418
221.263862	7196.032125	26.632436
221.357698	7211.221631	26.637453
221.252089	7221.938419	26.642471
221.895441	7220.245747	26.647488
222.130836	7234.388276	26.652506
222.446202	7238.988134	26.657524
222.653418	7246.762733	26.662541
222.902719	7247.197482	26.667559
223.467577	7261.407116	26.672576
223.129857	7275.434109	26.677594
223.196332	7276.882313	26.682612
223.675563	7276.085232	26.687629
223.875011	7293.178614	26.692647
224.250905	7295.623182	26.697664
224.435088	7303.952258	26.702682
224.410850	7304.231546	26.707700
224.459254	7319.566099	26.712717
224.424581	7333.201784	26.717735
225.026979	7350.651164	26.722752
225.348275	7356.090441	26.727770
225.644452	7359.110306	26.732788
225.559274	7353.587042	26.737805
225.623784	7382.547672	26.742823
226.067639	7381.390352	26.747840
226.134041	7400.123564	26.752858
226.888483	7398.206230	26.757876
226.919119	7415.930159	26.762893
226.920672	7415.158858	26.767911
227.529211	7418.412989	26.772928
227.078971	7453.253151	26.777946
227.038531	7459.677800	26.782964
227.677039	7475.182037	26.787981
227.832499	7484.104341	26.792999
227.897667	7497.349731	26.798016
228.108845	7513.853734	26.803034
228.677976	7522.852538	26.808052
228.908530	7541.895741	26.813069
229.407942	7552.262965	26.818087
229.583331	7564.114671	26.823104
229.659139	7579.641046	26.828122
229.701005	7581.577894	26.833140
230.151900	7590.629421	26.838157
230.175234	7607.151668	26.843175
230.757128	7612.772963	26.848192
230.920099	7621.361320	26.853210
231.414338	7619.950459	26.858228
231.633413	7635.539820	26.863245
231.639372	7647.720747	26.868263
232.399368	7642.343556	26.873280
231.967456	7649.389343	26.878298
232.206400	7670.451190	26.883316
232.575098	7671.568783	26.888333
232.923561	7672.677012	26.893351
233.073394	7696.269416	26.898368
232.962857	7699.718490	26.903386
232.943565	7710.903024	26.908404
233.544194	7722.505314	26.913421
233.865858	7747.049242	26.918439
234.422880	7749.897781	26.923456
234.412524	7763.489068	26.928474
234.653855	7764.993641	26.933492
235.016683	7786.055576	26.938509
235.168401	7798.209458	26.943527
235.371380	7791.578642	26.948544
235.324747	7815.972088	26.953562
235.493860	7812.810367	26.958580
235.701163	7831.525597	26.963597
235.795449	7853.410987	26.968615
236.400037	7861.490028	26.973632
236.411100	7881.885054	26.978650
236.622830	7888.988875	26.983668
237.201663	7917.693095	26.988685
236.983387	7927.349572	26.993703
237.240249	7935.999470	26.998720
237.346813	7950.324524	27.003738
237.885453	7967.553461	27.008756
238.033886	7972.420937	27.013773
238.329121	7985.500257	27.018791
238.639152	8003.152022	27.023808
238.915786	8021.107352	27.028826
238.929850	8023.461790	27.033844
239.315903	8036.344915	27.038861
239.463749	8044.558235	27.043879
239.662806	8056.148472	27.048896
239.854882	8068.501513	27.053914
240.481973	8079.319299	27.058932
240.641855	8099.969452	27.063949
240.417742	8116.006868	27.068967
240.663526	8120.596849	27.073984
240.972008	8143.057555	27.079002
241.476945	8156.166549	27.084020
241.693058	8167.683337	27.089037
242.241018	8178.180178	27.094055
242.562095	8171.749906	27.099072
242.810695	8179.439712	27.104090
242.807532	8184.587153	27.109108
243.409987	8204.535052	27.114125
243.178415	8224.506543	27.119143
243.792606	8213.181629	27.124160
243.794780	8222.510442	27.129178
243.660274	8257.355657	27.134196
244.326849	8251.317223	27.139213
244.201575	8270.946855	27.144231
244.670199	8277.751820	27.149248
244.627034	8309.155767	27.154266
245.156697	8315.496207	27.159284
245.617105	8313.897895	27.164301
245.721770	8333.566498	27.169319
246.168964	8326.227676	27.174336
246.262928	8353.521257	27.179354
246.557071	8364.604781	27.184372
246.869793	8369.622461	27.189389
246.835431	8393.822111	27.194407
247.320778	8398.615566	27.199424
247.496748	8404.718128	27.204442
247.635225	8414.872018	27.209460
248.141256	8417.776031	27.214477
247.905245	8446.914892	27.219495
248.675089	8448.846768	27.224512
248.645916	8465.182402	27.229530
248.703608	8488.546027	27.234548
249.513916	8491.748572	27.239565
249.414544	8488.076325	27.244583
249.642558	8506.119465	27.249600
249.914998	8528.014432	27.254618
250.247681	8526.111474	27.259636
250.605518	8538.856321	27.264653
250.530738	8553.132957	27.269671
250.866707	8557.295978	27.274688
251.104666	8565.184403	27.279706
251.145569	8568.591046	27.284724
251.901585	8582.915485	27.289741
251.398490	8594.652290	27.294759
251.953363	8603.327078	27.299776
251.939263	8618.909784	27.304794
251.858479	8636.148526	27.309812
252.608478	8642.418971	27.314829
253.145591	8652.243120	27.319847
253.061025	8665.395774	27.324864
253.487467	8687.084263	27.329882
253.833023	8686.550397	27.334900
254.278877	8693.553941	27.339917
254.358865	8713.814788	27.344935
254.317315	8721.909948	27.349952
254.528436	8739.797898	27.354970
254.919067	8750.723902	27.359988
255.547557	8768.123584	27.365005
255.432702	8782.995034	27.370023
255.729984	8794.261332	27.375040
256.011910	8811.619122	27.380058
256.050031	8815.562144	27.385076
256.359903	8828.615481	27.390093
256.385226	8854.403379	27.395111
256.973980	8870.671653	27.400128
257.289566	8878.749712	27.405146
257.274013	8902.669803	27.410164
258.149476	8906.621816	27.415181
258.171672	8921.197715	27.420199
258.226306	8932.024354	27.425216
258.377724	8960.626382	27.430234
259.045923	8968.194635	27.435252
259.446247	8971.818320	27.440269
259.507944	8985.442121	27.445287
259.982212	8996.051229	27.450304
259.934242	9004.055889	27.455322
260.007418	9021.146595	27.460340
260.411674	9033.540194	27.465357
260.514634	9048.450372	27.470375
260.799777	9059.723135	27.475392
261.513774	9075.222136	27.480410
261.624465	9095.596644	27.485428
261.810781	9089.735943	27.490445
262.332910	9114.960758	27.495463
262.908543	9118.021041	27.500480
262.999250	9131.865803	27.505498
262.724260	9134.132712	27.510516
263.485529	9128.331443	27.515533
263.412491	9144.866425	27.520551
263.751933	9152.408875	27.525568
263.921013	9155.488324	27.530586
263.887373	9176.136973	27.535604
264.353629	9185.412878	27.540621
264.293624	9214.103387	27.545639
264.457617	9224.892348	27.550656
264.946302	9234.545185	27.555674
265.108713	9248.959376	27.560692
265.781615	9258.043825	27.565709
265.717059	9272.769244	27.570727
266.124804	9281.132652	27.575744
266.381951	9299.257490	27.580762
266.498588	9303.268786	27.585780
266.751102	9329.642177	27.590797
266.904228	9333.585892	27.595815
267.356229	9341.163222	27.600832
267.925103	9342.227012	27.605850
267.738470	9377.486442	27.610868
268.610042	9389.895959	27.615885
268.636445	9390.740887	27.620903
268.759265	9402.566238	27.625920
269.140551	9422.810320	27.630938
269.314169	9422.705172	27.635956
269.477272	9440.987606	27.640973
269.671793	9465.659686	27.645991
269.951545	9470.406782	27.651008
270.397295	9478.882679	27.656026
270.549401	9500.330025	27.661044
271.200964	9509.885471	27.666061
271.202244	9509.526855	27.671079
271.175586	9546.591207	27.676096
271.669517	9545.881394	27.681114
272.028962	9567.325301	27.686132
272.407611	9584.218837	27.691149
272.260503	9602.532417	27.696167
272.726033	9611.728044	27.701184
273.197880	9613.809493	27.706202
273.166556	9643.217090	27.711220
273.605113	9631.929737	27.716237
273.974928	9670.804130	27.721255
274.305403	9680.931034	27.726272
274.538240	9694.192177	27.731290
274.737719	9700.319855	27.736308
275.325231	9705.100212	27.741325
275.337088	9729.213203	27.746343
275.628278	9741.191410	27.751360
276.098992	9749.914521	27.756378
276.123553	9763.368671	27.761396
276.641310	9757.266804	27.766413
276.986567	9775.687842	27.771431
276.742690	9789.672316	27.776448
277.347565	9796.383870	27.781466
277.531470	9818.753240	27.786484
277.795431	9832.725280	27.791501
277.812437	9852.719518	27.796519
278.204650	9865.039789	27.801536
278.885742	9869.183196	27.806554
278.795671	9882.062358	27.811572
279.390981	9903.281072	27.816589
279.987224	9901.001878	27.821607
279.926836	9905.721483	27.826624
280.406819	9905.333385	27.831642
280.567145	9911.891954	27.836660
280.650986	9927.569798	27.841677
280.609349	9938.241739	27.846695
280.746442	9943.184855	27.851712
281.328268	9943.123640	27.856730
281.108055	9977.694157	27.861748
281.277641	9983.722444	27.866765
281.970146	9997.596825	27.871783
282.005338	10015.808666	27.876800
282.492391	10031.720221	27.881818
282.772585	10049.339818	27.886836
282.940850	10061.054960	27.891853
283.434658	10072.873259	27.896871
283.811454	10097.534249	27.901888
284.307665	10103.259877	27.906906
284.122655	10124.984953	27.911924
284.427913	10148.815764	27.916941
284.757350	10149.511312	27.921959
285.019313	10168.990026	27.926976
285.378328	10178.871513	27.931994
285.611566	10203.829817	27.937012
285.860099	10217.886521	27.942029
286.053949	10226.434865	27.947047
286.317329	10269.542025	27.952064
286.898649	10273.966662	27.957082
287.019894	10291.888893	27.962100
287.291196	10307.041459	27.967117
287.907636	10324.534994	27.972135
287.791400	10340.230991	27.977152
288.618365	10357.842900	27.982170
288.551686	10364.725095	27.987188
288.930200	10379.442761	27.992205
289.065836	10397.654401	27.997223
289.302080	10419.295449	28.002240
289.720009	10425.844667	28.007258
289.690793	10453.282901	28.012276
290.219472	10465.079821	28.017293
290.534449	10479.117130	28.022311
290.800270	10498.904549	28.027328
291.323961	10526.856451	28.032346
291.565382	10541.888099	28.037364
292.020612	10548.386961	28.042381
292.289968	10560.368912	28.047399
292.144137	10588.990728	28.052416
292.942250	10571.812177	28.057434
293.092654	10616.748421	28.062452
293.238591	10608.313404	28.067469
293.948661	10600.584135	28.072487
293.741677	10654.354407	28.077504
294.460798	10637.825052	28.082522
294.317836	10652.277063	28.087540
294.539269	10684.101448	28.092557
295.349371	10686.827608	28.097575
294.962944	10701.960659	28.102592
295.694203	10706.326116	28.107610
295.828946	10729.584545	28.112628
296.020933	10752.024454	28.117645
296.462516	10753.450206	28.122663
296.650588	10764.641352	28.127680
296.867961	10771.939647	28.132698
297.092337	10793.175850	28.137716
297.329033	10808.018456	28.142733
297.778522	10823.247424	28.147751
297.707908	10854.495406	28.152768
298.404252	10860.235867	28.157786
298.423875	10882.407526	28.162804
298.782070	10903.409278	28.167821
299.458658	10919.453302	28.172839
299.737824	10927.642165	28.177856
299.419004	10934.830027	28.182874
300.120306	10964.984437	28.187892
300.365600	10979.083688	28.192909
300.804471	10983.413584	28.197927
300.805184	11009.690953	28.202944
301.823589	11012.310786	28.207962
301.944400	11050.552783	28.212980
302.057347	11051.613428	28.217997
302.307267	11069.755331	28.223015
302.877834	11080.763767	28.228032
303.129490	11084.003207	28.233050
303.400884	11108.890036	28.238068
303.517125	11118.464154	28.243085
304.020826	11131.370167	28.248103
304.319747	11157.513105	28.253120
304.477154	11158.722109	28.258138
304.631479	11181.784900	28.263156
304.803461	11194.051251	28.268173
305.446541	11211.815858	28.273191
305.937815	11219.013660	28.278208
305.856118	11230.224929	28.283226
306.281165	11265.349578	28.288244
306.518394	11279.411832	28.293261
307.246083	11289.285670	28.298279
307.318600	11298.829486	28.303296
307.850526	11314.410605	28.308314
308.183676	11324.300908	28.313332
308.199204	11341.634829	28.318349
308.639875	11351.870837	28.323367
308.892487	11373.319792	28.328384
309.235923	11387.270383	28.333402
309.227888	11398.571171	28.338420
309.400517	11416.005279	28.343437
309.890811	11432.075608	28.348455
310.222120	11449.675717	28.353472
310.770578	11477.051295	28.358490
310.774754	11483.353285	28.363508
310.904523	11512.947422	28.368525
311.508845	11518.287249	28.373543
311.446475	11545.628469	28.378560
311.974812	11559.308917	28.383578
312.229220	11580.501305	28.388596
312.274803	11594.034018	28.393613
312.915011	11595.339660	28.398631
312.987591	11621.978716	28.403648
313.391353	11641.518199	28.408666
314.075327	11663.674066	28.413684
314.080405	11673.520469	28.418701
314.414098	11686.295857	28.423719
314.730149	11708.619037	28.428736
315.326487	11706.442680	28.433754
315.295916	11727.338716	28.438772
315.467964	11761.624522	28.443789
315.959108	11770.305030	28.448807
316.007100	11796.147482	28.453824
316.676390	11809.885189	28.458842
316.748527	11837.199990	28.463860
316.951335	11855.571511	28.468877
317.416683	11865.291562	28.473895
317.563423	11890.051774	28.478912
318.393992	11909.864188	28.483930
318.506715	11932.155367	28.488948
318.676117	11952.042704	28.493965
319.610857	11949.065264	28.498983
319.652865	11976.612186	28.504000
319.926132	11991.351945	28.509018
320.588035	12012.631313	28.514036
320.112947	12031.862730	28.519053
320.761743	12045.995880	28.524071
321.315140	12067.186166	28.529088
321.934804	12081.273423	28.534106
322.236710	12093.140235	28.539124
322.397191	12105.682275	28.544141
322.369831	12114.345654	28.549159
322.488732	12139.558753	28.554176
322.899700	12154.362911	28.559194
323.531856	12176.542549	28.564212
323.636678	12205.902747	28.569229
323.940599	12214.721375	28.574247
324.189682	12229.289505	28.579264
324.503284	12251.678419	28.584282
324.867908	12275.330371	28.589300
325.531408	12299.138586	28.594317
326.069196	12301.044043	28.599335
326.286886	12333.720191	28.604352
326.527822	12354.500034	28.609370
326.813265	12354.498463	28.614388
326.833549	12376.908135	28.619405
327.138439	12399.001924	28.624423
327.405880	12421.366372	28.629440
328.039377	12428.045835	28.634458
328.320714	12450.227670	28.639476
328.533722	12472.817909	28.644493
329.294408	12480.765989	28.649511
329.330187	12495.659395	28.654528
329.495085	12507.662102	28.659546
329.814911	12530.462874	28.664564
330.013673	12545.175888	28.669581
330.925665	12558.375603	28.674599
331.086629	12571.432123	28.679616
331.236215	12588.223867	28.684634
331.482136	12607.605181	28.689652
331.482999	12631.204481	28.694669
331.666099	12630.366398	28.699687
332.250177	12655.479070	28.704704
332.357359	12682.502517	28.709722
333.102233	12683.751443	28.714740
333.485268	12713.921704	28.719757
333.481742	12736.807177	28.724775
333.648905	12752.753903	28.729792
334.205306	12771.934825	28.734810
334.476187	12791.566042	28.739828
334.700639	12833.664074	28.744845
335.258456	12847.022414	28.749863
335.534124	12870.454127	28.754880
335.844080	12892.273126	28.759898
336.197597	12908.249549	28.764916
336.477413	12932.765734	28.769933
337.310069	12953.288974	28.774951
337.375890	12976.688961	28.779968
337.704374	12990.085155	28.784986
338.135110	13009.392469	28.790004
338.139513	13032.542776	28.795021
338.918261	13052.499750	28.800039
339.110997	13077.593821	28.805056
339.125281	13100.504356	28.810074
339.884812	13120.121689	28.815092
340.113622	13133.532910	28.820109
340.840641	13143.484633	28.825127
340.791385	13168.130973	28.830144
341.258954	13189.351663	28.835162
341.727668	13208.842484	28.840180
341.859776	13228.808281	28.845197
342.377711	13247.390633	28.850215
342.796735	13259.911910	28.855232
342.905627	13272.082755	28.860250
343.685342	13300.440976	28.865268
343.608608	13317.606486	28.870285
344.087209	13329.495506	28.875303
344.297450	13346.497641	28.880320
344.881678	13372.700877	28.885338
345.453926	13377.769416	28.890356
345.478236	13416.187826	28.895373
345.823841	13407.358931	28.900391
346.185363	13435.806874	28.905408
346.413713	13443.793071	28.910426
346.665842	13477.144707	28.915444
347.045538	13496.476813	28.920461
347.377287	13517.243581	28.925479
347.483928	13532.831599	28.930496
347.804431	13549.765915	28.935514
348.044419	13554.857550	28.940532
348.225136	13576.082184	28.945549
348.746826	13607.435676	28.950567
349.236305	13634.797308	28.955584
349.313096	13657.549061	28.960602
350.089376	13659.249920	28.965620
350.194155	13676.432858	28.970637
350.704786	13688.946289	28.975655
351.070528	13713.477887	28.980672
351.152400	13742.040432	28.985690
351.519215	13751.442765	28.990708
351.748192	13784.279730	28.995725
352.246960	13800.040996	29.000743
352.709092	13825.881911	29.005760
352.711496	13847.150784	29.010778
353.344378	13872.142205	29.015796
353.502863	13906.191092	29.020813
354.171428	13923.784025	29.025831
354.235595	13936.200055	29.030848
354.528494	13972.883082	29.035866
355.312201	13992.848086	29.040884
355.589793	14018.344533	29.045901
356.214862	14038.005543	29.050919
356.528758	14061.300361	29.055936
356.897287	14070.585527	29.060954
357.303496	14100.139967	29.065972
357.364233	14118.982999	29.070989
357.925213	14130.158345	29.076007
358.006526	14149.753630	29.081024
358.434724	14184.063713	29.086042
359.060693	14197.470544	29.091060
358.892574	14224.150251	29.096077
359.301921	14248.959837	29.101095
359.771679	14260.831515	29.106112
360.092005	14298.956816	29.111130
360.478745	14312.591385	29.116148
361.141444	14347.725554	29.121165
361.263574	14361.966843	29.126183
361.564613	14382.658211	29.131200
361.884014	14406.230262	29.136218
362.794902	14417.765308	29.141236
363.128984	14442.429469	29.146253
363.376867	14461.391292	29.151271
364.103743	14481.585919	29.156288
364.289014	14491.036729	29.161306
364.673348	14514.476487	29.166324
364.982198	14534.399103	29.171341
365.312539	14552.459940	29.176359
365.816737	14568.672204	29.181376
365.807031	14584.960666	29.186394
366.205475	14594.396563	29.191412
366.364238	14621.911166	29.196429
366.804260	14639.579528	29.201447
367.481417	14647.944239	29.206464
367.697675	14673.082650	29.211482
367.854482	14697.424354	29.216500
367.984916	14707.690234	29.221517
368.404321	14714.851775	29.226535
369.137807	14742.267832	29.231552
369.017542	14766.423660	29.236570
369.562116	14780.428283	29.241588
369.531431	14807.626641	29.246605
369.947733	14834.233867	29.251623
370.350305	14864.452610	29.256640
370.461206	14896.949845	29.261658
371.078486	14918.700344	29.266676
371.328077	14946.151659	29.271693
371.666454	14971.711059	29.276711
372.228233	15000.192890	29.281728
372.400189	15039.661293	29.286746
373.280588	15049.611490	29.291764
373.346821	15077.333638	29.296781
373.719819	15108.167774	29.301799
374.459052	15135.521727	29.306816
374.679518	15161.671761	29.311834
374.852428	15183.734534	29.316852
375.244922	15220.652073	29.321869
376.153268	15230.043527	29.326887
376.954372	15243.503676	29.331904
377.102706	15258.595282	29.336922
377.864294	15275.441160	29.341940
377.999366	15290.978518	29.346957
378.112940	15301.016036	29.351975
378.884113	15310.717921	29.356992
379.039385	15349.690081	29.362010
379.260508	15350.294812	29.367028
379.318195	15379.919070	29.372045
379.835809	15402.908924	29.377063
379.919156	15418.217300	29.382080
380.298955	15453.514226	29.387098
380.620357	15480.269660	29.392116
381.066385	15501.195591	29.397133
381.551468	15528.043017	29.402151
381.834258	15558.038070	29.407168
382.027005	15590.590451	29.412186
382.607959	15604.827886	29.417204
382.993220	15649.057944	29.422221
383.464982	15670.308685	29.427239
384.094020	15678.024179	29.432256
384.295539	15714.486124	29.437274
384.644070	15721.031693	29.442292
385.270794	15756.827769	29.447309
385.697983	15779.301688	29.452327
386.271299	15794.084515	29.457344
386.017701	15818.810289	29.462362
386.691180	15825.534205	29.467380
386.957249	15856.317506	29.472397
387.142885	15891.060355	29.477415
387.922908	15903.404659	29.482432
387.856189	15920.099322	29.487450
388.326851	15938.131270	29.492468
388.703972	15962.787974	29.497485
388.601659	16000.249933	29.502503
389.284528	16023.475369	29.507520
389.681381	16057.543508	29.512538
390.354470	16072.257959	29.517556
390.732830	16087.676763	29.522573
391.001987	16108.881372	29.527591
391.586313	16125.442803	29.532608
391.757105	16164.264380	29.537626
392.567706	16188.049351	29.542644
393.281204	16194.377844	29.547661
393.416765	16222.710899	29.552679
393.684830	16234.525325	29.557696
393.786195	16259.398465	29.562714
394.249791	16286.941881	29.567732
394.651403	16312.596478	29.572749
394.756181	16329.842916	29.577767
395.525924	16345.549766	29.582784
395.873751	16380.232055	29.587802
396.067023	16399.741716	29.592820
396.681421	16423.592758	29.597837
397.014396	16445.161038	29.602855
397.776838	16460.896922	29.607872
397.816795	16496.519353	29.612890
398.349701	16512.424523	29.617908
398.532044	16542.356803	29.622925
399.025590	16571.225511	29.627943
399.596333	16577.714886	29.632960
400.004963	16623.471292	29.637978
399.950241	16635.493540	29.642996
400.367712	16660.484657	29.648013
401.152825	16693.492267	29.653031
401.350147	16720.389793	29.658048
401.531859	16746.373423	29.663066
402.274005	16773.246827	29.668084
402.841672	16797.930804	29.673101
402.828049	16837.351900	29.678119
403.712945	16846.949654	29.683136
403.851431	16875.783586	29.688154
404.546216	16901.962670	29.693172
404.850455	16921.651551	29.698189
405.115972	16942.277239	29.703207
405.649686	16963.146810	29.708224
405.952467	16997.334172	29.713242
406.428221	17018.809057	29.718260
406.895235	17036.332791	29.723277
407.147952	17065.302995	29.728295
407.868994	17086.121431	29.733312
407.872419	17109.540225	29.738330
407.979766	17138.883304	29.743348
408.610010	17165.838997	29.748365
408.969420	17208.825107	29.753383
409.292282	17217.513713	29.758400
409.494563	17251.659387	29.763418
409.847302	17267.904454	29.768436
410.301057	17301.850934	29.773453
410.447612	17340.584064	29.778471
411.122237	17353.140221	29.783488
411.770571	17372.366617	29.788506
412.266034	17413.152844	29.793524
412.589215	17431.198136	29.798541
412.988729	17466.264368	29.803559
413.498837	17492.238857	29.808576
413.769590	17516.016041	29.813594
414.169492	17540.672430	29.818612
414.719525	17558.988205	29.823629
414.773156	17587.418308	29.828647
415.576275	17620.309297	29.833664
415.881260	17641.366614	29.838682
416.480856	17670.594677	29.843700
416.855550	17695.372646	29.848717
417.052283	17724.432725	29.853735
417.759104	17748.457112	29.858752
417.913421	17779.129877	29.863770
418.323874	17805.019988	29.868788
419.010330	17819.369836	29.873805
419.086814	17856.176530	29.878823
419.939236	17873.377816	29.883840
420.402117	17907.068081	29.888858
420.293190	17927.495303	29.893876
421.060266	17952.393446	29.898893
421.089330	17987.337997	29.903911
421.895661	18012.967359	29.908928
422.040996	18038.828842	29.913946
422.619001	18062.729366	29.918964
423.446186	18093.632549	29.923981
423.467033	18132.429023	29.928999
424.375381	18147.254049	29.934016
424.645066	18173.914824	29.939034
425.022247	18199.878611	29.944052
425.260463	18226.306306	29.949069
425.631123	18246.181564	29.954087
426.029503	18281.802177	29.959104
426.441564	18312.666426	29.964122
426.603166	18333.549106	29.969140
427.500895	18359.582194	29.974157
427.553179	18393.751133	29.979175
428.269483	18426.841922	29.984192
428.875082	18455.665004	29.989210
429.064513	18485.989085	29.994228
429.440013	18508.376501	29.999245
430.202353	18535.621219	30.004263
430.718999	18561.627173	30.009280
431.186762	18581.838968	30.014298
431.277881	18610.001386	30.019316
431.877884	18636.268203	30.024333
432.021790	18660.628970	30.029351
432.408725	18674.305676	30.034368
433.109767	18702.301799	30.039386
433.105923	18726.910621	30.044404
433.228272	18747.075298	30.049421
433.556308	18784.877988	30.054439
434.278280	18815.577326	30.059456
434.642272	18849.281456	30.064474
434.948667	18884.248012	30.069492
435.656227	18903.620037	30.074509
435.698802	18950.049526	30.079527
436.321953	18970.763464	30.084544
436.522135	19013.078151	30.089562
437.130303	19050.356921	30.094580
437.667930	19074.105985	30.099597
438.314870	19103.024869	30.104615
438.698802	19136.025629	30.109632
439.325109	19158.124803	30.114650
439.428204	19197.643141	30.119668
440.055938	19224.958550	30.124685
440.573026	19265.102079	30.129703
441.135126	19297.257042	30.134720
441.339263	19327.447735	30.139738
441.677604	19349.671015	30.144756
442.201761	19384.029956	30.149773
442.605086	19423.299054	30.154791
443.356151	19450.546784	30.159808
443.860212	19476.043252	30.164826
443.823923	19508.034123	30.169844
444.867587	19519.576901	30.174861
445.057569	19572.454069	30.179879
445.664636	19601.634975	30.184896
446.307666	19618.108525	30.189914
446.547122	19641.494513	30.194932
447.332098	19661.633555	30.199949
447.561670	19697.539834	30.204967
448.074965	19716.444181	30.209984
448.515730	19742.026372	30.215002
448.774304	19769.629520	30.220020
449.409129	19798.559898	30.225037
449.749997	19828.046650	30.230055
450.498387	19853.268573	30.235072
450.942755	19869.715767	30.240090
451.253093	19912.288596	30.245108
451.749773	19934.272506	30.250125
451.706533	19962.046528	30.255143
452.533967	19994.094119	30.260160
452.768850	20018.281475	30.265178
452.895107	20049.762079	30.270196
453.438537	20086.941034	30.275213
454.241573	20111.732975	30.280231
454.602199	20153.087302	30.285248
455.144276	20170.208296	30.290266
455.386726	20207.516598	30.295284
456.056116	20220.995324	30.300301
456.239668	20252.920013	30.305319
456.570505	20281.660319	30.310336
456.922011	20313.493802	30.315354
457.191887	20343.662599	30.320372
457.956630	20373.667964	30.325389
457.930208	20416.513554	30.330407
458.630925	20437.846304	30.335424
459.277229	20480.184063	30.340442
459.604664	20507.946858	30.345460
459.891786	20540.260409	30.350477
460.412818	20574.555927	30.355495
460.765529	20604.580517	30.360512
461.360047	20631.999763	30.365530
461.510489	20684.609783	30.370548
462.268306	20705.486891	30.375565
463.116792	20749.984817	30.380583
463.078002	20783.304861	30.385600
463.835145	20828.565700	30.390618
463.963944	20862.358501	30.395636
464.235773	20888.362847	30.400653
464.917410	20932.515373	30.405671
465.783142	20964.431279	30.410688
466.545721	20990.420225	30.415706
467.045255	21020.461206	30.420724
467.286656	21059.397552	30.425741
468.103222	21082.258649	30.430759
468.146206	21114.577625	30.435776
468.877623	21149.704809	30.440794
469.323460	21187.377991	30.445812
469.853958	21203.705767	30.450829
470.204737	21234.241014	30.455847
470.807014	21265.949855	30.460864
471.490828	21278.590440	30.465882
471.149046	21321.158755	30.470900
471.829240	21350.347820	30.475917
472.213796	21382.564893	30.480935
473.047777	21427.021376	30.485952
473.367303	21448.387880	30.490970
473.509513	21479.082835	30.495988
474.411394	21504.251083	30.501005
474.605820	21546.786566	30.506023
475.385724	21581.020997	30.511040
476.269661	21612.502170	30.516058
476.538002	21643.834964	30.521076
477.104136	21671.355848	30.526093
477.771234	21702.000702	30.531111
478.175779	21724.854344	30.536128
478.685379	21749.547571	30.541146
479.062213	21791.038700	30.546164
479.715156	21807.501965	30.551181
479.936512	21844.891156	30.556199
480.244293	21869.330046	30.561216
480.745742	21884.262862	30.566234
481.018889	21920.619353	30.571252
481.579361	21948.146350	30.576269
482.030042	21992.070874	30.581287
482.178946	22020.016391	30.586304
482.658458	22038.699353	30.591322
483.332388	22083.621084	30.596340
483.999938	22106.256967	30.601357
483.663390	22134.701373	30.606375
484.034622	22182.247000	30.611392
484.717824	22214.360711	30.616410
485.013954	22251.554659	30.621428
485.773689	22296.780728	30.626445
485.817129	22335.796657	30.631463
486.567807	22371.399215	30.636480
487.165270	22411.752626	30.641498
487.679170	22458.258783	30.646516
488.461568	22487.610893	30.651533
488.918219	22529.905631	30.656551
489.161101	22555.602697	30.661568
489.906658	22592.849513	30.666586
490.394628	22627.034276	30.671604
490.848287	22662.809247	30.676621
491.251739	22694.758996	30.681639
491.855915	22742.184928	30.686656
492.353414	22784.070582	30.691674
492.808259	22818.060193	30.696692
493.512739	22847.509661	30.701709
493.979026	22901.047900	30.706727
494.388370	22930.232638	30.711744
495.028794	22967.014272	30.716762
495.434057	23012.220882	30.721780
496.079360	23036.701544	30.726797
496.334734	23064.391721	30.731815
496.894696	23112.466150	30.736832
497.515400	23148.414095	30.741850
497.697476	23181.446855	30.746868
498.461294	23220.606985	30.751885
499.090761	23249.435892	30.756903
499.635358	23293.763374	30.761920
499.890027	23321.304462	30.766938
500.667625	23361.734000	30.771956
500.893296	23404.939005	30.776973
501.453238	23443.241334	30.781991
501.933233	23477.285066	30.787008
502.692193	23512.780974	30.792026
502.768385	23561.194536	30.797044
503.633309	23581.210509	30.802061
504.137302	23628.081642	30.807079
504.509576	23664.309780	30.812096
504.647602	23696.488142	30.817114
505.242524	23739.595070	30.822132
505.838665	23772.254342	30.827149
506.592476	23815.588221	30.832167
506.905637	23843.042918	30.837184
507.684089	23878.557021	30.842202
508.051911	23921.547022	30.847220
508.636141	23957.521520	30.852237
509.436237	23979.927887	30.857255
509.640040	24014.494097	30.862272
510.280524	24036.551035	30.867290
510.734981	24078.607655	30.872308
511.161731	24112.239824	30.877325
511.479382	24141.515441	30.882343
512.065765	24169.333627	30.887360
512.494768	24199.560465	30.892378
512.524764	24244.214390	30.897396
513.469745	24268.435765	30.902413
514.078974	24310.831471	30.907431
514.489954	24345.016453	30.912448
514.833474	24381.828973	30.917466
515.702358	24408.264289	30.922484
515.923321	24447.583238	30.927501
516.273082	24487.240959	30.932519
516.661011	24523.166085	30.937536
517.229806	24565.376712	30.942554
517.600299	24622.807579	30.947572
518.167227	24659.245654	30.952589
518.906387	24708.908027	30.957607
519.116097	24745.615092	30.962624
520.007816	24781.759888	30.967642
520.231442	24826.892678	30.972660
521.052382	24882.993965	30.977677
521.595555	24917.334781	30.982695
522.152802	24946.338187	30.987712
522.823658	24992.558162	30.992730
523.320919	25023.931287	30.997748
523.957824	25065.043752	31.002765
524.854785	25095.756257	31.007783
524.861805	25142.034349	31.012800
525.366057	25184.958767	31.017818
526.175680	25222.602520	31.022836
526.612172	25260.000152	31.027853
527.206693	25297.729546	31.032871
527.542377	25344.011804	31.037888
528.203435	25365.775849	31.042906
528.601626	25413.261475	31.047924
529.108127	25450.344332	31.052941
529.621786	25493.797448	31.057959
529.684427	25549.253014	31.062976
530.608411	25574.743285	31.067994
531.260792	25621.974775	31.073012
531.799429	25673.093200	31.078029
532.330620	25705.985785	31.083047
532.815857	25749.488238	31.088064
533.383098	25791.707872	31.093082
533.703528	25830.387321	31.098100
534.656630	25869.597885	31.103117
535.228398	25900.052569	31.108135
535.694492	25952.900779	31.113152
536.294140	25980.469507	31.118170
536.736754	26025.863065	31.123188
536.993417	26055.422114	31.128205
537.651706	26092.524037	31.133223
538.191388	26115.048950	31.138240
538.730655	26160.340839	31.143258
539.366542	26196.969177	31.148276
539.728624	26220.522223	31.153293
540.335858	26267.368918	31.158311
540.753467	26306.401935	31.163328
541.428481	26337.868285	31.168346
541.977878	26375.212728	31.173364
542.254952	26421.820975	31.178381
543.067607	26442.739890	31.183399
543.549010	26481.047853	31.188416
543.934424	26511.080398	31.193434
544.508795	26556.101538	31.198452
544.749634	26597.364533	31.203469
545.480134	26634.566504	31.208487
545.892057	26681.011434	31.213504
546.372847	26716.576124	31.218522
547.397359	26765.794509	31.223540
547.479342	26811.640057	31.228557
548.115016	26849.888878	31.233575
548.677871	26905.010265	31.238592
549.324502	26935.274585	31.243610
549.847610	26991.596934	31.248628
550.421689	27033.414597	31.253645
551.142478	27068.164259	31.258663
551.553304	27113.840907	31.263680
552.303768	27150.372028	31.268698
552.834706	27188.702152	31.273716
553.133562	27229.403682	31.278733
553.630134	27273.074693	31.283751
554.053863	27326.270574	31.288768
554.983408	27368.204243	31.293786
555.381740	27421.762952	31.298804
555.530020	27474.166501	31.303821
556.643330	27504.565560	31.308839
556.962269	27566.507488	31.313856
557.647523	27619.490146	31.318874
558.384858	27653.830331	31.323892
558.932123	27703.129172	31.328909
559.496375	27736.534339	31.333927
560.162543	27786.477875	31.338944
560.952534	27828.382971	31.343962
561.632342	27858.903742	31.348980
562.074384	27894.235332	31.353997
562.834195	27925.310752	31.359015
563.007757	27977.550394	31.364032
563.530531	28030.780884	31.369050
564.288663	28064.412699	31.374068
564.535208	28108.162034	31.379085
564.959846	28140.361184	31.384103
565.596634	28199.197948	31.389120
566.166433	28243.923566	31.394138
566.777576	28277.667478	31.399156
566.825274	28326.288262	31.404173
568.090664	28366.258054	31.409191
568.502531	28405.527137	31.414208
568.994378	28438.002969	31.419226
569.847989	28468.468851	31.424244
570.241485	28497.451185	31.429261
571.062249	28533.418783	31.434279
571.381601	28576.346253	31.439296
572.004560	28613.136582	31.444314
572.501895	28652.079067	31.449332
572.748436	28692.170958	31.454349
573.498540	28734.362102	31.459367
574.034780	28768.487710	31.464384
574.465189	28814.133744	31.469402
575.167083	28854.353646	31.474420
575.482132	28890.287542	31.479437
576.409476	28934.568898	31.484455
576.388618	28988.667577	31.489472
577.356295	29025.971248	31.494490
578.104406	29067.533242	31.499508
578.593093	29123.306714	31.504525
578.871659	29167.789732	31.509543
579.909228	29208.702437	31.514560
580.360200	29250.287007	31.519578
580.986561	29295.521829	31.524596
581.404141	29353.263070	31.529613
582.033648	29387.591023	31.534631
582.414631	29440.511488	31.539648
583.039980	29486.066907	31.544666
583.929043	29530.620738	31.549684
583.905722	29578.610462	31.554701
584.926031	29637.128194	31.559719
585.673947	29681.515809	31.564736
585.885375	29725.647010	31.569754
586.932215	29771.054157	31.574772
587.467706	29817.475809	31.579789
588.107561	29858.313235	31.584807
588.688269	29923.574467	31.589824
589.286439	29967.302757	31.594842
590.329026	29998.283548	31.599860
590.444804	30052.031476	31.604877
590.906599	30090.809718	31.609895
591.561198	30131.478432	31.614912
592.050186	30178.269410	31.619930
592.834737	30227.495590	31.624948
593.170254	30278.005343	31.629965
594.050010	30319.548002	31.634983
594.593239	30364.133977	31.640000
595.008871	30410.138285	31.645018
595.780226	30458.472109	31.650036
596.070774	30515.618337	31.655053
596.904822	30560.013544	31.660071
597.866455	30610.407283	31.665088
598.030031	30649.568455	31.670106
598.859702	30696.922884	31.675124
599.208235	30737.581962	31.680141
599.879478	30776.475050	31.685159
600.533100	30827.309359	31.690176
601.073404	30880.062554	31.695194
602.069551	30907.738104	31.700212
602.208675	30951.970814	31.705229
602.810258	30990.628069	31.710247
603.326491	31029.425089	31.715264
603.810952	31079.456550	31.720282
604.571844	31111.740430	31.725300
604.871309	31159.100254	31.730317
605.517462	31206.527939	31.735335
606.077393	31255.414737	31.740352
606.672220	31311.719380	31.745370
607.461198	31349.458742	31.750388
607.663923	31410.529149	31.755405
608.212649	31456.721672	31.760423
608.548734	31522.433295	31.765440
609.358427	31566.947020	31.770458
610.127169	31626.760216	31.775476
610.569062	31688.424007	31.780493
611.534373	31740.787619	31.785511
612.203875	31794.725753	31.790528
612.516835	31852.429439	31.795546
613.354917	31893.341261	31.800564
613.946544	31952.088444	31.805581
614.251700	32009.319510	31.810599
615.612638	32062.741779	31.815616
615.886280	32109.897255	31.820634
616.719527	32164.321198	31.825652
617.271977	32217.239104	31.830669
618.233771	32265.168089	31.835687
618.688417	32314.938541	31.840704
619.041902	32370.330094	31.845722
619.872449	32411.651059	31.850740
620.452381	32472.170423	31.855757
621.283606	32513.709049	31.860775
621.874979	32563.056555	31.865792
622.401256	32612.598987	31.870810
623.011075	32657.385503	31.875828
623.431833	32732.687488	31.880845
624.172625	32778.381859	31.885863
624.976237	32819.958756	31.890880
625.019867	32879.718593	31.895898
625.835525	32935.046328	31.900916
626.508106	32993.052970	31.905933
626.926129	33051.600015	31.910951
627.847775	33101.407240	31.915968
628.401219	33151.665729	31.920986
629.642378	33196.067878	31.926004
630.013142	33267.170115	31.931021
630.533175	33308.998315	31.936039
631.440121	33358.969436	31.941056
631.767121	33410.248355	31.946074
632.513057	33439.608927	31.951092
632.975125	33511.443249	31.956109
633.962199	33553.249716	31.961127
634.573089	33592.810090	31.966144
634.635579	33647.386883	31.971162
635.666673	33677.894146	31.976180
636.186263	33729.045656	31.981197
636.941202	33762.035575	31.986215
637.493526	33816.516012	31.991232
637.760071	33864.659666	31.996250
638.898707	33895.939938	32.001268
639.071529	33948.260217	32.006285
639.571347	34001.085034	32.011303
640.328925	34055.951301	32.016320
640.688628	34110.636773	32.021338
641.641750	34164.597401	32.026356
642.032766	34232.149070	32.031373
642.829461	34274.536245	32.036391
643.508122	34321.010881	32.041408
643.948084	34378.408389	32.046426
644.758569	34423.303307	32.051444
645.432586	34490.369584	32.056461
646.044408	34549.526341	32.061479
646.716046	34600.516033	32.066496
647.244663	34655.293054	32.071514
647.595460	34711.197310	32.076532
648.413884	34772.407524	32.081549
649.169889	34835.894764	32.086567
649.864395	34896.570275	32.091584
650.490658	34959.727107	32.096602
651.398484	35007.355790	32.101620
652.111345	35063.624484	32.106637
652.724390	35119.750042	32.111655
653.579385	35174.833078	32.116672
654.311840	35233.433920	32.121690
654.971594	35268.037349	32.126708
655.783675	35334.009913	32.131725
656.475443	35382.889514	32.136743
657.291094	35429.930305	32.141760
657.467543	35492.799771	32.146778
658.057601	35537.021813	32.151796
658.796565	35587.032706	32.156813
659.641658	35635.029458	32.161831
660.475820	35690.979851	32.166848
660.726391	35756.021931	32.171866
661.812063	35790.322158	32.176884
662.176127	35856.964037	32.181901
662.758919	35909.767514	32.186919
663.542080	35958.093510	32.191936
663.955223	36025.466051	32.196954
664.611684	36065.135414	32.201972
665.468564	36131.029901	32.206989
665.924153	36183.335819	32.212007
666.831731	36227.819712	32.217024
667.359263	36292.993199	32.222042
668.064771	36340.848670	32.227060
668.117413	36400.537727	32.232077
669.100185	36470.212983	32.237095
669.957679	36516.759868	32.242112
670.421187	36571.865705	32.247130
671.291141	36625.398235	32.252148
671.758102	36669.125758	32.257165
672.340657	36733.437695	32.262183
673.243021	36771.122509	32.267200
673.613121	36843.444620	32.272218
674.328700	36878.559622	32.277236
674.865480	36945.772707	32.282253
675.332003	37008.650549	32.287271
676.325285	37045.254145	32.292288
676.705924	37125.014223	32.297306
677.507127	37173.221034	32.302324
678.528172	37234.262964	32.307341
679.312708	37292.966789	32.312359
679.952411	37342.148930	32.317376
680.621522	37399.714256	32.322394
681.478779	37457.820569	32.327412
681.948914	37516.496400	32.332429
682.347042	37564.861532	32.337447
683.627182	37627.340966	32.342464
684.055894	37684.775263	32.347482
684.625705	37745.097827	32.352500
685.400225	37804.265421	32.357517
685.874168	37858.424654	32.362535
686.280447	37933.856486	32.367552
687.423516	37987.405062	32.372570
687.805596	38040.415904	32.377588
688.806082	38104.420580	32.382605
689.580885	38164.429778	32.387623
690.483703	38213.927336	32.392640
691.148700	38281.506904	32.397658
691.855009	38339.436896	32.402676
692.687559	38392.008170	32.407693
693.311936	38449.741879	32.412711
694.202693	38497.856239	32.417728
694.923208	38562.607302	32.422746
695.633862	38606.600644	32.427764
696.260148	38668.853772	32.432781
696.363964	38731.065745	32.437799
697.295576	38777.640206	32.442816
698.330632	38828.782008	32.447834
698.923350	38901.285634	32.452852
699.694875	38944.197954	32.457869
700.322448	39011.920427	32.462887
701.034969	39053.133177	32.467904
701.686195	39124.428504	32.472922
702.616149	39187.119271	32.477940
702.952681	39240.265693	32.482957
703.590820	39298.162518	32.487975
704.836654	39345.232521	32.492992
704.789115	39410.227364	32.498010
705.396598	39469.028444	32.503028
706.231682	39521.591789	32.508045
706.901655	39587.922196	32.513063
707.797970	39654.850720	32.518080
707.884563	39709.932199	32.523098
709.108255	39757.371128	32.528116
709.679664	39810.527671	32.533133
710.186192	39879.493369	32.538151
711.404618	39933.712600	32.543168
711.639132	39988.782470	32.548186
712.376517	40045.369847	32.553204
713.247797	40103.500372	32.558221
713.897202	40160.417517	32.563239
714.916147	40212.783428	32.568256
715.117879	40289.212325	32.573274
715.723766	40336.965690	32.578292
716.709748	40394.968567	32.583309
717.348678	40480.099542	32.588327
718.109388	40535.877450	32.593344
718.640066	40600.324314	32.598362
719.321467	40660.525950	32.603380
720.260109	40731.190904	32.608397
720.748958	40793.762280	32.613415
721.387868	40855.559363	32.618432
722.319100	40935.013169	32.623450
722.891283	40989.554691	32.628468
723.956929	41063.635452	32.633485
724.119815	41138.607739	32.638503
725.393502	41193.047698	32.643520
726.061496	41248.990934	32.648538
726.656930	41315.127035	32.653556
727.453904	41403.486076	32.658573
728.184618	41465.400063	32.663591
728.950046	41536.300934	32.668608
730.024401	41599.728264	32.673626
730.636618	41661.403192	32.678644
731.400222	41726.470112	32.683661
732.120706	41798.994115	32.688679
732.736535	41861.369396	32.693696
733.383816	41932.748061	32.698714
734.170678	41993.390216	32.703732
735.175043	42064.406634	32.708749
735.927766	42126.297427	32.713767
736.811346	42196.835264	32.718784
737.466243	42261.634490	32.723802
737.674180	42322.571834	32.728820
738.865269	42384.135130	32.733837
739.492143	42455.692698	32.738855
740.216774	42528.165498	32.743872
741.022207	42584.138526	32.748890
741.392784	42651.148288	32.753908
742.236354	42720.786220	32.758925
742.785492	42804.230264	32.763943
743.845058	42861.920675	32.768960
744.644402	42932.083806	32.773978
745.394016	43008.626857	32.778996
746.575316	43067.891510	32.784013
747.481736	43128.575417	32.789031
748.370832	43178.565899	32.794048
748.547024	43228.512292	32.799066
749.295839	43280.436940	32.804084
750.377797	43332.614688	32.809101
750.762220	43387.313582	32.814119
751.690170	43431.434611	32.819136
752.111250	43500.808583	32.824154
752.537924	43561.709175	32.829172
753.367078	43608.962950	32.834189
753.814348	43691.629429	32.839207
754.456517	43761.073348	32.844224
755.180171	43827.772807	32.849242
756.078192	43890.192531	32.854260
757.189168	43962.546769	32.859277
757.532298	44040.427201	32.864295
758.540743	44095.697756	32.869312
759.153466	44174.072143	32.874330
759.710032	44262.395790	32.879348
760.719342	44328.701553	32.884365
761.497377	44398.060153	32.889383
762.190866	44474.804747	32.894400
763.064649	44535.839486	32.899418
763.848725	44614.545056	32.904436
764.714528	44675.370197	32.909453
765.423922	44760.072628	32.914471
766.511903	44830.440422	32.919488
767.321182	44895.631902	32.924506
767.624885	44971.702546	32.929524
768.426643	45035.980894	32.934541
769.557862	45112.327386	32.939559
770.179404	45192.209753	32.944576
770.741626	45264.653617	32.949594
771.510483	45328.304182	32.954612
772.413506	45398.110624	32.959629
772.918917	45483.962673	32.964647
774.124024	45539.585098	32.969664
775.241235	45623.684196	32.974682
775.917029	45700.257189	32.979700
777.068720	45764.170200	32.984717
777.802964	45821.190342	32.989735
778.739343	45892.271160	32.994752
779.377181	45961.087280	32.999770
779.755997	46025.657440	33.004788
780.621290	46081.266278	33.009805
781.058753	46159.242124	33.014823
782.043442	46228.622446	33.019840
782.764441	46310.683601	33.024858
783.476845	46372.510801	33.029876
784.385768	46443.367921	33.034893
785.143192	46517.079435	33.039911
786.035714	46594.325401	33.044928
786.717453	46653.360019	33.049946
787.529457	46731.875089	33.054964
788.438435	46800.231738	33.059981
788.893621	46879.738145	33.064999
789.906834	46940.494090	33.070016
790.454302	47000.936307	33.075034
790.878001	47069.021035	33.080052
792.094994	47126.612225	33.085069
792.920435	47203.306796	33.090087
793.621350	47259.220032	33.095104
794.389539	47321.638012	33.100122
794.872330	47402.480150	33.105140
795.705808	47470.722069	33.110157
796.518068	47548.941015	33.115175
797.169122	47623.753163	33.120192
798.217153	47689.772108	33.125210
798.849256	47771.131707	33.130228
799.802487	47836.639378	33.135245
800.410640	47908.708240	33.140263
801.207444	47982.053630	33.145280
801.790476	48058.926186	33.150298
802.648811	48138.866328	33.155316
803.864784	48222.823348	33.160333
804.441370	48304.553942	33.165351
805.280015	48387.246585	33.170368
806.146784	48449.517195	33.175386
806.570924	48531.809504	33.180404
808.038321	48615.655804	33.185421
808.453481	48681.987445	33.190439
809.327099	48769.652283	33.195456
810.276332	48841.342507	33.200474
811.135264	48937.722487	33.205492
812.162908	49002.771424	33.210509
812.748738	49075.485987	33.215527
813.722669	49144.302086	33.220544
814.699946	49225.310520	33.225562
815.397737	49312.027841	33.230580
816.421993	49382.263120	33.235597
817.250738	49449.273342	33.240615
818.049635	49543.031345	33.245632
818.600011	49615.283594	33.250650
819.617212	49685.158312	33.255668
820.851844	49755.888560	33.260685
821.110812	49828.484674	33.265703
821.889280	49906.403872	33.270720
823.047582	49975.739766	33.275738
823.687971	50068.162559	33.280756
824.736016	50132.038515	33.285773
825.565605	50206.482891	33.290791
826.446639	50283.099926	33.295808
827.402248	50347.796053	33.300826
827.961950	50424.471148	33.305844
829.095993	50492.443367	33.310861
829.756910	50567.370510	33.315879
830.571721	50638.376203	33.320896
831.432001	50702.123149	33.325914
832.372963	50791.535501	33.330932
833.108414	50857.092156	33.335949
833.914535	50916.648219	33.340967
834.376602	50994.628840	33.345984
834.920564	51054.530036	33.351002
835.920146	51120.490584	33.356020
836.709149	51188.753897	33.361037
837.222575	51260.425405	33.366055
837.972943	51340.403451	33.371072
838.939575	51414.417644	33.376090
839.557478	51504.064853	33.381108
840.351759	51581.625927	33.386125
841.266327	51660.597800	33.391143
841.980060	51741.886840	33.396160
843.143419	51821.103855	33.401178
843.587208	51902.799512	33.406196
844.380902	51981.905649	33.411213
845.634343	52075.667728	33.416231
846.337381	52155.944133	33.421248
847.312561	52245.459287	33.426266
847.959967	52336.081149	33.431284
848.859250	52406.250384	33.436301
850.176511	52496.454008	33.441319
850.883429	52575.822737	33.446336
852.175208	52646.732081	33.451354
852.449746	52741.461363	33.456372
853.716487	52822.594693	33.461389
854.440378	52903.398176	33.466407
854.835598	52992.182444	33.471424
856.388903	53072.475960	33.476442
857.014756	53156.998301	33.481460
857.652670	53238.659652	33.486477
858.517491	53324.170492	33.491495
859.564941	53409.122437	33.496512
860.172701	53491.496712	33.501530
861.099387	53584.387571	33.506548
862.440756	53667.236112	33.511565
863.169199	53759.098927	33.516583
863.871813	53841.406044	33.521600
865.218156	53926.625324	33.526618
865.658407	53999.635534	33.531636
866.641516	54076.757513	33.536653
867.536846	54167.920397	33.541671
868.488748	54244.883929	33.546688
869.166482	54326.717448	33.551706
869.751859	54422.738028	33.556724
870.877148	54488.529942	33.561741
872.073864	54583.582934	33.566759
872.835227	54671.891052	33.571776
873.834752	54743.338062	33.576794
874.439798	54835.484785	33.581812
875.135262	54911.466114	33.586829
876.188545	54996.427725	33.591847
876.911656	55084.784968	33.596864
878.021074	55166.708238	33.601882
878.766802	55255.337321	33.606900
879.666545	55344.882967	33.611917
880.666204	55416.828171	33.616935
881.362324	55499.270086	33.621952
882.529248	55567.486655	33.626970
883.155711	55652.528715	33.631988
883.798828	55727.139198	33.637005
884.815702	55802.028266	33.642023
885.681322	55886.007465	33.647040
886.612846	55961.387414	33.652058
887.213430	56053.613598	33.657076
887.962568	56129.765071	33.662093
889.112134	56206.497101	33.667111
889.542355	56303.474009	33.672128
890.470878	56384.677085	33.677146
891.339042	56482.743757	33.682164
892.171071	56570.832000	33.687181
893.376362	56653.826281	33.692199
894.313634	56747.097763	33.697216
895.151875	56836.287997	33.702234
896.149923	56934.295376	33.707252
897.170272	57020.723756	33.712269
898.235119	57098.319022	33.717287
898.938076	57190.903976	33.722304
900.023382	57279.450936	33.727322
900.936068	57363.808233	33.732340
901.575174	57450.807551	33.737357
902.472060	57536.307782	33.742375
903.614538	57638.785021	33.747392
904.659835	57723.271237	33.752410
905.529961	57806.188307	33.757428
906.386828	57895.639578	33.762445
907.854182	57977.035447	33.767463
908.202063	58068.153335	33.772480
909.239250	58143.405461	33.777498
910.704004	58218.308887	33.782516
911.461867	58311.061204	33.787533
912.282670	58390.471830	33.792551
913.186204	58470.952499	33.797568
914.378753	58556.915539	33.802586
914.969482	58639.625083	33.807604
915.647328	58734.640089	33.812621
916.763991	58811.669201	33.817639
917.594100	58906.016809	33.822656
918.416757	58994.399101	33.827674
919.212713	59075.142611	33.832692
920.010412	59174.838634	33.837709
921.121593	59273.184554	33.842727
921.776731	59365.042905	33.847744
923.116273	59443.027379	33.852762
923.695985	59535.094317	33.857780
924.612100	59633.028010	33.862797
925.700871	59709.888483	33.867815
926.415589	59818.204675	33.872832
927.517756	59903.162219	33.877850
928.791235	59997.460606	33.882868
929.166142	60088.435707	33.887885
930.406329	60179.548265	33.892903
930.954952	60271.904790	33.897920
932.132623	60346.136303	33.902938
932.954739	60424.387186	33.907956
933.658309	60513.272399	33.912973
934.875092	60597.359217	33.917991
935.306285	60690.045916	33.923008
936.298498	60772.729471	33.928026
937.619373	60849.630334	33.933044
938.439662	60947.358833	33.938061
939.370123	61028.660903	33.943079
939.979806	61127.251107	33.948096
941.316698	61213.866527	33.953114
942.197828	61297.782557	33.958132
943.051893	61398.043520	33.963149
944.121429	61483.326036	33.968167
944.798690	61577.016802	33.973184
945.745115	61668.129671	33.978202
946.530480	61768.896126	33.983220
947.765248	61872.187182	33.988237
948.684539	61964.354133	33.993255
949.481876	62066.749617	33.998272
950.562403	62152.118675	34.003290
951.544778	62253.598432	34.008308
952.386710	62345.204855	34.013325
953.432740	62442.169467	34.018343
954.324320	62555.415146	34.023360
955.822657	62635.143367	34.028378
957.115713	62736.004739	34.033396
957.964473	62815.473927	34.038413
959.053487	62901.050283	34.043431
960.140937	63003.818366	34.048448
961.110561	63082.170530	34.053466
961.912987	63174.513559	34.058484
962.704195	63269.675627	34.063501
963.872656	63351.534065	34.068519
964.371391	63451.243532	34.073536
965.591109	63542.448287	34.078554
966.400223	63627.172456	34.083572
967.605921	63722.994018	34.088589
968.487693	63806.226360	34.093607
969.368505	63908.198527	34.098624
970.515905	63993.069462	34.103642
971.458568	64085.252506	34.108660
972.552812	64187.148002	34.113677
973.768589	64276.427372	34.118695
974.526127	64374.600450	34.123712
975.239143	64461.885846	34.128730
976.376874	64549.151445	34.133748
977.124306	64647.239109	34.138765
978.106276	64751.511414	34.143783
979.141076	64851.019765	34.148800
980.174433	64931.134803	34.153818
981.460634	65021.796040	34.158836
982.112195	65133.775173	34.163853
983.322858	65211.819854	34.168871
983.870279	65305.142294	34.173888
984.851661	65386.944511	34.178906
985.579165	65473.966938	34.183924
986.682213	65549.143508	34.188941
987.759885	65647.357470	34.193959
988.254991	65745.320362	34.198976
989.356465	65829.704615	34.203994
990.588687	65923.319066	34.209012
991.211021	66022.892812	34.214029
992.177013	66116.995883	34.219047
993.253017	66223.980565	34.224064
994.205463	66317.654081	34.229082
995.206051	66408.120967	34.234100
995.928694	66511.243925	34.239117
997.244850	66611.686287	34.244135
997.907804	66716.411673	34.249152
999.084016	66816.037224	34.254170
1000.227444	66924.625878	34.259188
1000.945564	67040.203012	34.264205
1002.128730	67127.485762	34.269223
1003.189599	67232.854994	34.274240
1004.003635	67349.382064	34.279258
1005.138067	67450.691556	34.284276
1006.175141	67561.915984	34.289293
1007.637939	67662.498420	34.294311
1008.264461	67776.846891	34.299328
1009.048519	67876.521345	34.304346
1010.800451	67974.140854	34.309364
1011.387580	68088.958592	34.314381
1012.650383	68192.734241	34.319399
1014.045353	68299.313280	34.324416
1015.067833	68400.058035	34.329434
1016.086113	68486.198110	34.334452
1017.181733	68587.854547	34.339469
1018.028617	68683.764271	34.344487
1019.032432	68794.944202	34.349504
1020.106287	68888.885673	34.354522
1021.541909	68980.287243	34.359540
1022.124519	69089.691127	34.364557
1023.327256	69184.662247	34.369575
1024.337244	69303.835919	34.374592
1025.452840	69383.362512	34.379610
1026.122554	69489.197912	34.384628
1027.147820	69595.135271	34.389645
1028.402723	69697.549247	34.394663
1029.349939	69800.183285	34.399680
1030.097839	69898.686088	34.404698
1031.945171	69986.147714	34.409716
1032.822046	70097.879644	34.414733
1033.771344	70190.621514	34.419751
1035.019053	70281.818991	34.424768
1035.939305	70384.030755	34.429786
1037.183059	70477.548489	34.434804
1037.965732	70576.523021	34.439821
1039.407194	70665.562269	34.444839
1040.286197	70746.376708	34.449856
1040.675482	70832.804093	34.454874
1041.860574	70910.341934	34.459892
1042.512899	71001.308912	34.464909
1043.411424	71095.788010	34.469927
1044.393608	71191.915964	34.474944
1045.490859	71293.339790	34.479962
1046.164233	71392.569591	34.484980
1046.925990	71499.867045	34.489997
1048.261688	71591.903272	34.495015
1049.281103	71713.162516	34.500032
1050.159326	71829.219570	34.505050
1051.660040	71920.062161	34.510068
1052.527365	72040.311366	34.515085
1053.612360	72145.602160	34.520103
1054.444951	72246.889742	34.525120
1055.515771	72374.918432	34.530138
1056.469171	72473.445656	34.535156
1057.551907	72598.263996	34.540173
1058.522517	72702.842972	34.545191
1059.801490	72818.045912	34.550208
1060.898832	72933.126757	34.555226
1062.361323	73048.124916	34.560244
1063.241545	73156.979584	34.565261
1064.293280	73267.741166	34.570279
1065.296738	73394.864578	34.575296
1066.631696	73494.498872	34.580314
1067.705816	73602.876487	34.585332
1068.273519	73725.344661	34.590349
1069.641855	73833.108014	34.595367
1070.934438	73947.007265	34.600384
1072.214207	74066.760784	34.605402
1073.061060	74176.890166	34.610420
1074.106644	74289.693194	34.615437
1075.038217	74402.375966	34.620455
1076.379772	74516.871010	34.625472
1077.247944	74636.731320	34.630490
1078.654624	74751.381651	34.635508
1079.489837	74873.043329	34.640525
1080.395145	74979.275040	34.645543
1082.103612	75100.438998	34.650560
1083.054410	75208.168732	34.655578
1084.294914	75322.772923	34.660596
1085.309992	75438.721783	34.665613
1086.442847	75536.780566	34.670631
1087.734929	75641.829364	34.675648
1088.853105	75762.162199	34.680666
1090.232516	75856.581080	34.685684
1090.980260	75976.898273	34.690701
1091.949688	76079.352671	34.695719
1093.461706	76189.652727	34.700736
1094.235537	76298.263295	34.705754
1095.170834	76409.863375	34.710772
1096.163355	76516.285236	34.715789
1097.351558	76612.766774	34.720807
1098.181680	76720.112973	34.725824
1099.223306	76823.804707	34.730842
1100.458470	76917.726925	34.735860
1100.886335	77025.062871	34.740877
1102.172738	77119.186437	34.745895
1103.521255	77229.145274	34.750912
1104.454365	77343.550687	34.755930
1105.594735	77449.018536	34.760948
1106.659040	77562.911338	34.765965
1107.776304	77669.452135	34.770983
1108.951583	77790.009147	34.776000
1110.055911	77889.626035	34.781018
1111.187387	78015.443596	34.786036
1111.893634	78116.079284	34.791053
1112.859706	78239.933587	34.796071
1114.146414	78353.548939	34.801088
1115.335803	78481.850456	34.806106
1116.519251	78604.964497	34.811124
1117.454064	78710.768631	34.816141
1118.846113	78839.640626	34.821159
1120.177633	78952.778130	34.826176
1121.156971	79073.310667	34.831194
1122.510042	79189.656998	34.836212
1123.580734	79316.952334	34.841229
1124.611407	79430.778723	34.846247
1126.159514	79543.215029	34.851264
1126.798850	79665.069290	34.856282
1128.329736	79783.874842	34.861300
1129.636983	79899.973324	34.866317
1130.592077	80011.646839	34.871335
1131.951815	80122.991125	34.876352
1133.102304	80238.844640	34.881370
1134.220334	80363.743217	34.886388
1134.420994	80471.462048	34.891405
1135.918692	80598.691079	34.896423
1137.316135	80719.710391	34.901440
1138.543484	80835.321142	34.906458
1139.882193	80957.040204	34.911476
1141.174061	81091.068829	34.916493
1142.094372	81195.661688	34.921511
1143.262648	81334.749705	34.926528
1144.233273	81444.677445	34.931546
1145.571672	81542.251935	34.936564
1146.651944	81674.497380	34.941581
1147.393106	81793.598104	34.946599
1149.033612	81910.413466	34.951616
1150.379485	82028.249873	34.956634
1151.498973	82161.067445	34.961652
1152.671861	82263.033612	34.966669
1153.782341	82384.203087	34.971687
1154.763956	82491.201306	34.976704
1155.647727	82622.896088	34.981722
1156.891809	82733.204388	34.986740
1158.031889	82869.512867	34.991757
1159.136545	82985.989574	34.996775
1160.973635	83096.806082	35.001792
1162.120673	83191.738205	35.006810
1163.131551	83279.832994	35.011828
1164.094459	83388.103184	35.016845
1165.193570	83491.439999	35.021863
1166.476352	83597.011443	35.026880
1167.196464	83711.125626	35.031898
1168.613246	83812.036372	35.036916
1169.507581	83928.501179	35.041933
1170.904262	84036.427559	35.046951
1172.145058	84159.363134	35.051968
1172.675747	84275.685370	35.056986
1173.785479	84394.558927	35.062004
1174.996646	84503.731096	35.067021
1176.170881	84633.040359	35.072039
1177.446438	84747.261507	35.077056
1178.522909	84870.872250	35.082074
1180.262640	84980.095612	35.087092
1180.959810	85125.391282	35.092109
1182.543498	85243.075154	35.097127
1184.059947	85350.818504	35.102144
1185.066129	85482.144994	35.107162
1185.977089	85607.594645	35.112180
1187.340082	85726.062374	35.117197
1188.273095	85844.080661	35.122215
1190.074642	85976.029832	35.127232
1190.724903	86098.558418	35.132250
1191.981946	86213.251980	35.137268
1193.101252	86355.586722	35.142285
1194.347350	86477.630726	35.147303
1196.049308	86593.128166	35.152320
1197.032898	86716.195343	35.157338
1198.146853	86846.931393	35.162356
1199.133053	86969.778307	35.167373
1200.632299	87099.569403	35.172391
1201.733479	87234.881513	35.177408
1202.832330	87361.993585	35.182426
1204.249567	87465.925198	35.187444
1205.361805	87606.163734	35.192461
1206.301156	87735.807418	35.197479
1208.049569	87868.314219	35.202496
1208.922525	87992.898642	35.207514
1210.108908	88124.079928	35.212532
1211.473723	88249.466597	35.217549
1212.767318	88386.981251	35.222567
1214.334751	88500.246532	35.227584
1214.891155	88631.063120	35.232602
1216.566479	88762.619535	35.237620
1217.568907	88889.540957	35.242637
1218.562387	89024.470403	35.247655
1220.104640	89150.656188	35.252672
1220.977302	89267.166224	35.257690
1222.496638	89411.430638	35.262708
1223.735294	89541.499225	35.267725
1224.698205	89659.774037	35.272743
1226.225495	89775.366941	35.277760
1227.102600	89904.375844	35.282778
1228.464726	90012.489685	35.287796
1229.500419	90125.632998	35.292813
1230.479787	90263.551026	35.297831
1232.205498	90380.285564	35.302848
1233.362025	90497.705690	35.307866
1234.373056	90614.896611	35.312884
1235.771260	90737.705776	35.317901
1236.752512	90869.138665	35.322919
1237.845782	90981.081976	35.327936
1239.050145	91116.364008	35.332954
1240.424923	91230.237039	35.337972
1241.656279	91356.807594	35.342989
1242.977670	91492.263077	35.348007
1244.208305	91616.254868	35.353024
1245.302830	91774.004060	35.358042
1246.544033	91896.857338	35.363060
1247.975617	92030.508771	35.368077
1248.861589	92166.113528	35.373095
1250.182857	92308.676650	35.378112
1251.354770	92453.123910	35.383130
1252.761767	92592.582446	35.388148
1254.343207	92726.201630	35.393165
1255.254450	92875.525252	35.398183
1256.798534	92997.779934	35.403200
1258.346409	93127.921872	35.408218
1259.361125	93287.459233	35.413236
1260.692847	93430.432733	35.418253
1262.060727	93556.361722	35.423271
1263.459429	93683.842498	35.428288
1264.401802	93829.391524	35.433306
1265.614953	93969.692845	35.438324
1267.424422	94105.573817	35.443341
1268.466251	94241.463795	35.448359
1269.681865	94363.873107	35.453376
1270.849419	94532.528811	35.458394
1272.103403	94644.452504	35.463412
1273.790243	94783.241469	35.468429
1274.941945	94944.438840	35.473447
1276.494546	95071.479293	35.478464
1277.605695	95189.032795	35.483482
1278.810297	95348.055014	35.488500
1280.529316	95456.777703	35.493517
1281.421792	95610.727677	35.498535
1282.857302	95753.275759	35.503552
1283.934643	95860.919511	35.508570
1285.324610	96036.028703	35.513588
1286.492494	96159.891371	35.518605
1287.445167	96303.101664	35.523623
1289.085440	96426.182216	35.528640
1289.902977	96588.020156	35.533658
1291.427230	96728.611932	35.538676
1293.030650	96863.081102	35.543693
1294.060684	97005.429546	35.548711
1295.271486	97115.727658	35.553728
1296.613531	97253.555550	35.558746
1297.694652	97389.673418	35.563764
1299.305936	97503.692787	35.568781
1300.396197	97630.327738	35.573799
1301.990709	97747.545729	35.578816
1303.223458	97895.219528	35.583834
1304.504417	98011.925687	35.588852
1305.806778	98129.008624	35.593869
1306.694821	98281.927318	35.598887
1308.056206	98409.200433	35.603904
1309.562372	98537.950614	35.608922
1310.463812	98685.460773	35.613940
1311.868981	98821.921619	35.618957
1313.085557	98970.130054	35.623975
1314.433050	99101.856816	35.628992
1315.959034	99243.381237	35.634010
1316.672833	99390.723313	35.639028
1318.325111	99535.791389	35.644045
1319.568990	99689.744802	35.649063
1320.835162	99841.487649	35.654080
1322.305715	99989.795169	35.659098
1323.503326	100153.907308	35.664116
1325.113349	100293.235738	35.669133
1326.456208	100443.939078	35.674151
1327.881668	100586.436795	35.679168
1329.197709	100738.228238	35.684186
1330.160085	100888.292649	35.689204
1331.970381	101033.636094	35.694221
1333.395128	101192.778025	35.699239
1334.997831	101333.493220	35.704256
1336.047934	101478.156724	35.709274
1337.567941	101631.003562	35.714292
1338.776158	101789.798038	35.719309
1340.099011	101924.025155	35.724327
1341.410702	102060.336538	35.729344
1343.325020	102215.990868	35.734362
1344.475332	102375.368013	35.739380
1346.039753	102504.390516	35.744397
1347.230982	102651.930566	35.749415
1348.497474	102801.155384	35.754432
1349.850890	102945.539341	35.759450
1351.321651	103094.062831	35.764468
1353.031079	103246.061222	35.769485
1354.099031	103395.479575	35.774503
1355.737836	103525.837380	35.779520
1357.137580	103675.641402	35.784538
1357.864936	103823.870024	35.789556
1359.629056	103954.400128	35.794573
1360.924625	104119.790227	35.799591
1362.467071	104252.103731	35.804608
1363.286547	104395.088046	35.809626
1364.829984	104542.653604	35.814644
1366.255709	104694.092615	35.819661
1367.252918	104860.528833	35.824679
1368.832174	104978.032655	35.829696
1370.299187	105112.160172	35.834714
1371.157613	105231.488432	35.839732
1372.812414	105374.466144	35.844749
1373.692236	105507.815911	35.849767
1375.092003	105652.329315	35.854784
1376.654252	105794.514231	35.859802
1378.040805	105941.771696	35.864820
1379.591862	106079.928873	35.869837
1380.759105	106234.608347	35.874855
1382.111506	106365.603213	35.879872
1383.454736	106516.086019	35.884890
1384.632004	106672.962761	35.889908
1386.318737	106795.065735	35.894925
1387.651958	106959.545629	35.899943
1389.150383	107112.646598	35.904960
1390.729637	107265.235723	35.909978
1391.766221	107410.083282	35.914996
1393.461709	107570.440348	35.920013
1394.715359	107726.242256	35.925031
1395.885283	107876.463673	35.930048
1397.208010	108036.579290	35.935066
1398.531290	108196.499680	35.940084
1400.250279	108349.864604	35.945101
1401.689005	108511.945941	35.950119
1402.893384	108663.299689	35.955136
1404.428602	108823.456370	35.960154
1405.802654	108988.279061	35.965172
1407.475786	109135.757388	35.970189
1408.637054	109298.046304	35.975207
1410.349195	109464.476785	35.980224
1412.026087	109630.496264	35.985242
1413.359948	109785.153040	35.990260
1414.834010	109938.503629	35.995277
1416.442397	110094.504902	36.000295
1417.343939	110255.486939	36.005312
1418.709790	110409.433671	36.010330
1419.931870	110576.323054	36.015348
1421.696350	110739.221956	36.020365
1422.844549	110903.568105	36.025383
1424.448883	111077.014738	36.030400
1425.990591	111238.895279	36.035418
1427.502725	111399.800454	36.040436
1428.956370	111571.343905	36.045453
1430.221235	111731.765154	36.050471
1431.777934	111887.760714	36.055488
1433.422460	112058.068186	36.060506
1434.729414	112224.752691	36.065524
1436.500400	112378.735982	36.070541
1437.799834	112538.910099	36.075559
1438.875926	112700.057607	36.080576
1440.478373	112867.395801	36.085594
1441.705788	113033.971774	36.090612
1443.648184	113192.788213	36.095629
1444.698315	113354.342894	36.100647
1445.972572	113505.120300	36.105664
1447.531726	113656.461071	36.110682
1448.784409	113805.914326	36.115700
1450.516563	113952.165011	36.120717
1451.873462	114091.139059	36.125735
1453.024398	114259.210376	36.130752
1454.799933	114401.126661	36.135770
1456.279203	114538.678345	36.140788
1457.351760	114715.963640	36.145805
1459.058776	114871.377899	36.150823
1460.284721	115017.556958	36.155840
1461.748734	115169.035928	36.160858
1462.830703	115342.044491	36.165876
1464.680913	115501.700564	36.170893
1465.915888	115669.584343	36.175911
1467.527704	115841.226952	36.180928
1468.836342	116005.923096	36.185946
1470.094592	116180.720058	36.190964
1471.724954	116354.693034	36.195981
1473.064849	116524.123254	36.200999
1474.540651	116691.418386	36.206016
1476.105773	116869.571184	36.211034
1477.735209	117050.025933	36.216052
1479.654835	117216.329624	36.221069
1480.763627	117391.063665	36.226087
1482.564061	117565.847297	36.231104
1484.205003	117734.572921	36.236122
1485.548903	117904.340896	36.241140
1487.246760	118079.182315	36.246157
1488.522806	118248.988674	36.251175
1489.810943	118429.608668	36.256192
1491.723377	118587.893885	36.261210
1493.302090	118779.240348	36.266228
1494.869846	118944.477762	36.271245
1496.569593	119112.316631	36.276263
1497.872151	119283.607229	36.281280
1499.597235	119473.206980	36.286298
1500.911224	119639.616225	36.291316
1502.239639	119798.438542	36.296333
1503.868825	119966.794380	36.301351
1505.297370	120156.699511	36.306368
1506.957480	120313.572659	36.311386
1508.501213	120486.979454	36.316404
1510.090129	120666.915034	36.321421
1511.971677	120832.823813	36.326439
1513.296486	120999.151369	36.331456
1514.836237	121168.181390	36.336474
1516.527516	121326.347457	36.341492
1517.970767	121506.590571	36.346509
1519.372100	121676.025795	36.351527
1521.065796	121846.732818	36.356544
1522.704401	121999.338734	36.361562
1523.945191	122184.102064	36.366580
1526.044277	122344.147226	36.371597
1527.575785	122498.647490	36.376615
1528.780790	122647.247825	36.381632
1530.163980	122778.684424	36.386650
1531.581471	122935.003832	36.391668
1532.873255	123097.170275	36.396685
1534.207121	123242.067804	36.401703
1535.617805	123398.859652	36.406720
1536.943980	123559.174261	36.411738
1538.364365	123726.719723	36.416756
1539.798308	123891.718236	36.421773
1541.267697	124060.663926	36.426791
1542.420803	124242.871639	36.431808
1544.216280	124403.610745	36.436826
1545.731388	124598.176199	36.441844
1547.131740	124764.008732	36.446861
1548.784975	124946.407771	36.451879
1550.130032	125129.148331	36.456896
1552.052101	125309.569155	36.461914
1553.437094	125494.446501	36.466932
1555.242624	125674.280278	36.471949
1556.923503	125860.202467	36.476967
1558.565447	126048.754171	36.481984
1559.855633	126232.372262	36.487002
1561.667789	126407.269726	36.492020
1563.371703	126584.452934	36.497037
1564.808669	126767.012616	36.502055
1566.318745	126957.200316	36.507072
1568.219215	127132.924465	36.512090
1569.730694	127322.291105	36.517108
1571.261612	127501.445886	36.522125
1572.984088	127681.078119	36.527143
1574.588631	127867.127484	36.532160
1576.115401	128053.899865	36.537178
1577.977597	128234.539627	36.542196
1579.718678	128410.918026	36.547213
1581.439576	128588.782928	36.552231
1583.022876	128783.012790	36.557248
1584.935999	128945.533629	36.562266
1586.626975	129122.355260	36.567284
1587.777254	129302.697046	36.572301
1589.795731	129490.427198	36.577319
1591.407924	129651.581111	36.582336
1592.837879	129814.893240	36.587354
1594.613475	129993.227225	36.592372
1595.866567	130190.863948	36.597389
1597.687649	130361.718460	36.602407
1598.861890	130530.713066	36.607424
1600.534630	130715.617872	36.612442
1602.249001	130888.316901	36.617460
1604.064389	131066.081309	36.622477
1605.697463	131241.139233	36.627495
1607.200572	131420.957239	36.632512
1608.750097	131604.873930	36.637530
1610.333701	131786.163814	36.642548
1612.011474	131947.561267	36.647565
1613.525497	132120.261680	36.652583
1614.833412	132295.276443	36.657600
1616.501426	132452.953421	36.662618
1617.769150	132625.049872	36.667636
1619.271523	132799.390700	36.672653
1621.229439	132953.793572	36.677671
1622.704314	133129.559843	36.682688
1623.904295	133291.547645	36.687706
1625.449356	133475.109757	36.692724
1627.091210	133649.078871	36.697741
1628.723035	133824.013593	36.702759
1630.291475	134019.371687	36.707776
1631.784824	134185.296515	36.712794
1633.510739	134382.089193	36.717812
1634.891015	134568.712789	36.722829
1636.698805	134761.199666	36.727847
1638.205494	134948.578573	36.732864
1640.184582	135137.087421	36.737882
1641.775079	135338.938548	36.742900
1643.632376	135526.024771	36.747917
1645.816828	135713.579770	36.752935
1647.279649	135891.937135	36.757952
1649.593699	136072.377914	36.762970
1650.918414	136256.639002	36.767988
1652.422896	136437.704806	36.773005
1654.516245	136622.745828	36.778023
1656.161577	136803.816882	36.783040
1657.677165	136986.138831	36.788058
1659.209536	137162.288029	36.793076
1660.630913	137353.446880	36.798093
1662.422647	137529.899242	36.803111
1664.146197	137739.615229	36.808128
1665.787874	137914.636433	36.813146
1667.438764	138111.086103	36.818164
1668.771264	138304.318162	36.823181
1671.006826	138485.812753	36.828199
1672.309596	138687.555275	36.833216
1674.050099	138876.759767	36.838234
1675.680350	139072.395377	36.843252
1677.403798	139268.904573	36.848269
1679.511590	139460.614370	36.853287
1681.093024	139650.926247	36.858304
1683.179932	139835.912426	36.863322
1684.926524	140027.290360	36.868340
1686.226385	140222.504403	36.873357
1688.445660	140398.132880	36.878375
1689.865364	140584.281518	36.883392
1691.723669	140775.899961	36.888410
1693.487258	140957.218410	36.893428
1695.024565	141137.116418	36.898445
1696.798467	141323.352792	36.903463
1698.069752	141519.251490	36.908480
1699.789256	141693.674163	36.913498
1701.590377	141894.611387	36.918516
1702.680629	142090.656588	36.923533
1704.838338	142274.391783	36.928551
1706.143144	142456.856688	36.933568
1707.900388	142626.386502	36.938586
1709.665067	142813.850212	36.943604
1711.142027	142989.320099	36.948621
1712.677228	143165.301397	36.953639
1714.225996	143353.018160	36.958656
1715.929145	143527.745443	36.963674
1717.954797	143710.255459	36.968692
1719.557343	143910.907937	36.973709
1721.103297	144094.332933	36.978727
1722.808617	144287.011747	36.983744
1724.535305	144470.929955	36.988762
1726.310066	144665.197149	36.993780
1727.532979	144870.948138	36.998797
1729.854986	145075.714764	37.003815
1731.165983	145280.237655	37.008832
1733.253330	145456.524603	37.013850
1735.019192	145683.704895	37.018868
1736.595151	145872.852277	37.023885
1738.393742	146077.201566	37.028903
1740.248029	146277.880063	37.033920
1742.108471	146479.205333	37.038938
1743.920216	146696.637996	37.043956
1745.560924	146892.740307	37.048973
1747.655783	147095.870318	37.053991
1749.064516	147300.935935	37.059008
1750.660556	147492.827914	37.064026
1752.643348	147728.722438	37.069044
1754.449027	147925.172570	37.074061
1756.206883	148135.778437	37.079079
1758.258835	148350.192675	37.084096
1760.048367	148543.923732	37.089114
1761.630631	148754.422119	37.094132
1763.463924	148964.476379	37.099149
1765.325239	149168.734237	37.104167
1767.262358	149384.808957	37.109184
1768.894922	149583.172952	37.114202
1771.147790	149794.547824	37.119220
1772.598792	150011.718096	37.124237
1774.768766	150201.671655	37.129255
1776.393900	150402.754802	37.134272
1778.536900	150599.535396	37.139290
1780.389560	150814.149825	37.144308
1781.944023	151006.956839	37.149325
1784.168279	151196.235692	37.154343
1785.619619	151404.439436	37.159360
1787.186502	151608.328381	37.164378
1789.557729	151796.078718	37.169396
1790.849231	152000.711106	37.174413
1792.621679	152206.143202	37.179431
1794.725829	152398.262599	37.184448
1796.695544	152597.314080	37.189466
1798.432657	152793.081979	37.194484
1800.014348	152987.202167	37.199501
1801.715949	153191.523271	37.204519
1803.416729	153374.152844	37.209536
1805.099172	153556.659547	37.214554
1807.188346	153728.947097	37.219572
1808.547023	153921.497962	37.224589
1810.267261	154092.793628	37.229607
1811.903341	154269.935798	37.234624
1813.602220	154463.729023	37.239642
1815.645945	154656.657173	37.244660
1816.666332	154835.966745	37.249677
1818.604872	155044.280834	37.254695
1820.125516	155266.089833	37.259712
1821.983472	155466.799118	37.264730
1823.940312	155678.562984	37.269748
1825.575847	155885.370798	37.274765
1827.477369	156104.031044	37.279783
1829.412632	156326.884292	37.284800
1831.186603	156543.893904	37.289818
1833.437586	156741.200898	37.294836
1834.918913	156968.834589	37.299853
1837.116701	157180.392035	37.304871
1838.867456	157392.376785	37.309888
1840.533759	157616.219448	37.314906
1842.561022	157846.561917	37.319924
1844.574546	158050.571226	37.324941
1846.598387	158274.399448	37.329959
1848.358468	158490.472534	37.334976
1850.310365	158709.116018	37.339994
1852.205197	158926.070740	37.345012
1853.664601	159144.414716	37.350029
1856.311887	159360.529913	37.355047
1858.165658	159577.102101	37.360064
1859.863159	159801.283599	37.365082
1862.275731	159997.416880	37.370100
1864.223417	160208.487209	37.375117
1866.085661	160437.249830	37.380135
1867.868750	160644.354346	37.385152
1869.617723	160849.766201	37.390170
1871.738233	161059.444613	37.395188
1873.396006	161291.301412	37.400205
1875.320350	161489.549502	37.405223
1877.238610	161706.999544	37.410240
1878.961434	161918.686422	37.415258
1881.284597	162139.638377	37.420276
1882.960247	162365.107730	37.425293
1884.767326	162566.056265	37.430311
1886.783650	162769.965651	37.435328
1888.781558	162987.537643	37.440346
1890.665255	163204.241328	37.445364
1892.507308	163420.711960	37.450381
1894.656999	163624.668418	37.455399
1896.546818	163837.823897	37.460416
1898.231252	164047.817261	37.465434
1900.200892	164248.229363	37.470452
1901.869069	164471.747248	37.475469
1903.879545	164666.917282	37.480487
1905.491364	164873.997239	37.485504
1907.301500	165073.297735	37.490522
1909.657499	165253.995786	37.495540
1911.350990	165449.917845	37.500557
1912.994003	165635.360169	37.505575
1914.617214	165840.896438	37.510592
1916.834279	166021.645666	37.515610
1918.546214	166222.084061	37.520628
1920.358342	166447.861364	37.525645
1922.288116	166629.661120	37.530663
1924.451349	166836.867490	37.535680
1925.729720	167043.708098	37.540698
1927.846046	167250.607119	37.545716
1929.696717	167480.963285	37.550733
1931.570522	167692.469310	37.555751
1933.646976	167912.696120	37.560768
1935.119108	168133.755776	37.565786
1937.418340	168347.798137	37.570804
1939.078770	168576.986215	37.575821
1941.266669	168808.793664	37.580839
1942.858527	169029.459017	37.585856
1945.259938	169258.584348	37.590874
1947.554731	169485.850708	37.595892
1949.316299	169698.755615	37.600909
1951.657711	169919.522789	37.605927
1953.915943	170151.390636	37.610944
1955.530318	170368.026465	37.615962
1957.850967	170572.564498	37.620980
1959.978024	170805.053262	37.625997
1961.993591	171004.492017	37.631015
1964.113073	171238.620911	37.636032
1966.303039	171451.797299	37.641050
1968.153073	171669.696852	37.646068
1970.199814	171881.782040	37.651085
1972.036027	172097.707306	37.656103
1974.006813	172307.472794	37.661120
1975.668803	172520.129887	37.666138
1977.823853	172744.862394	37.671156
1979.989926	172967.869220	37.676173
1982.273505	173185.733745	37.681191
1984.204795	173415.795389	37.686208
1986.097141	173627.812973	37.691226
1988.367424	173823.090108	37.696244
1990.318688	174037.333192	37.701261
1992.229797	174264.586707	37.706279
1994.231561	174486.346841	37.711296
1996.517706	174712.528517	37.716314
1998.180475	174913.895111	37.721332
2000.133440	175140.093992	37.726349
2002.393001	175351.998984	37.731367
2004.452158	175559.179566	37.736384
2006.341830	175770.739477	37.741402
2008.408220	175977.007630	37.746420
2010.507977	176188.739359	37.751437
2012.479877	176405.820775	37.756455
2014.449915	176592.811254	37.761472
2016.387582	176787.229357	37.766490
2018.473915	176971.615053	37.771508
2019.966685	177158.607710	37.776525
2022.116184	177339.420075	37.781543
2024.019426	177538.909188	37.786560
2025.713040	177741.363182	37.791578
2028.027271	177922.748240	37.796596
2029.679143	178135.043125	37.801613
2031.235083	178352.162695	37.806631
2033.434363	178564.195294	37.811648
2035.383040	178759.166433	37.816666
2037.465531	178989.032481	37.821684
2039.323661	179204.979358	37.826701
2041.412567	179433.311649	37.831719
2043.922173	179635.708773	37.836736
2045.646225	179859.635278	37.841754
2048.048520	180094.125594	37.846772
2049.855075	180303.234969	37.851789
2051.916221	180524.129899	37.856807
2054.404084	180744.856771	37.861824
2056.240082	180971.702220	37.866842
2058.639235	181196.949667	37.871860
2060.531531	181419.461978	37.876877
2062.769389	181628.560139	37.881895
2064.929126	181867.120725	37.886912
2066.915301	182088.758795	37.891930
2069.381042	182308.609008	37.896948
2071.504324	182524.187958	37.901965
2073.519515	182749.301369	37.906983
2075.710648	182958.616349	37.912000
2077.996521	183178.118818	37.917018
2079.839919	183393.657625	37.922036
2082.168694	183611.734336	37.927053
2084.486479	183827.859815	37.932071
2086.362095	184038.283131	37.937088
2088.536933	184261.424877	37.942106
2091.100249	184465.980426	37.947124
2093.282502	184691.698983	37.952141
2095.247644	184905.436681	37.957159
2097.641941	185102.446654	37.962176
2099.384730	185317.160571	37.967194
2101.878624	185532.644604	37.972212
2103.695415	185732.400971	37.977229
2106.129183	185943.277639	37.982247
2108.236734	186163.089546	37.987264
2110.140026	186374.433043	37.992282
2112.342500	186565.033624	37.997300
2114.667157	186771.578972	38.002317
2116.787982	186985.187585	38.007335
2118.727112	187191.592947	38.012352
2120.913822	187401.944513	38.017370
2123.322437	187604.749537	38.022388
2125.272632	187798.275817	38.027405
2127.357670	187997.910694	38.032423
2129.456788	188189.333857	38.037440
2131.337551	188367.455348	38.042458
2133.378144	188536.859548	38.047476
2135.586930	188726.592451	38.052493
2137.530532	188904.249182	38.057511
2139.406098	189085.445227	38.062528
2141.233431	189286.852346	38.067546
2143.381840	189473.031910	38.072564
2145.510181	189678.466514	38.077581
2147.583535	189877.007201	38.082599
2149.970301	190064.496462	38.087616
2151.489032	190278.659804	38.092634
2153.715420	190496.975869	38.097652
2156.131751	190686.531438	38.102669
2157.912070	190904.755136	38.107687
2160.268025	191120.540758	38.112704
2162.027203	191341.003341	38.117722
2164.261389	191560.858581	38.122740
2166.562917	191772.125148	38.127757
2168.663279	192003.108083	38.132775
2171.114520	192219.264220	38.137792
2173.115168	192451.394587	38.142810
2175.366479	192671.125219	38.147828
2177.844309	192898.245207	38.152845
2179.554258	193115.842744	38.157863
2181.865726	193353.562955	38.162880
2184.470611	193560.220288	38.167898
2186.524894	193807.298862	38.172916
2189.186772	194027.998419	38.177933
2191.426298	194255.428947	38.182951
2193.855879	194468.323975	38.187968
2195.510006	194712.297611	38.192986
2197.802337	194908.463407	38.198004
2200.179604	195154.723218	38.203021
2202.371065	195368.713228	38.208039
2205.020063	195600.082789	38.213056
2207.367729	195824.761821	38.218074
2209.466082	196048.605639	38.223092
2211.788938	196266.157701	38.228109
2214.044136	196487.262486	38.233127
2216.271165	196706.887718	38.238144
2218.496609	196920.878837	38.243162
2220.396356	197158.796464	38.248180
2222.663085	197367.020634	38.253197
2224.880398	197579.797309	38.258215
2227.286572	197825.379964	38.263232
2229.571823	198043.097765	38.268250
2232.152743	198253.268352	38.273268
2234.458499	198476.175905	38.278285
2236.438803	198715.737861	38.283303
2238.748358	198911.205363	38.288320
2241.089331	199157.553433	38.293338
2243.066495	199345.345416	38.298356
2245.324079	199602.916421	38.303373
2247.689559	199794.875098	38.308391
2249.765144	199993.798035	38.313408
2251.711531	200210.981893	38.318426
2253.954865	200382.602625	38.323444
2256.178325	200579.409939	38.328461
2258.202234	200795.162235	38.333479
2260.447849	201000.878079	38.338496
2262.220506	201198.063748	38.343514
2264.467526	201405.494467	38.348532
2266.621597	201616.126709	38.353549
2268.466962	201849.072720	38.358567
2270.889227	202070.275759	38.363584
2273.055524	202288.093055	38.368602
2275.270889	202525.705185	38.373620
2277.293396	202764.605563	38.378637
2279.511951	202998.119200	38.383655
2282.389616	203233.128698	38.388672
2284.289361	203476.253153	38.393690
2286.317521	203733.600633	38.398708
2289.040928	203957.048251	38.403725
2291.331724	204202.931836	38.408743
2293.615000	204444.070167	38.413760
2295.923187	204689.902316	38.418778
2298.292280	204931.384522	38.423796
2300.544156	205199.099497	38.428813
2302.710894	205452.535664	38.433831
2305.506953	205691.071790	38.438848
2308.073112	205940.867012	38.443866
2310.235646	206194.637124	38.448884
2312.788121	206437.886404	38.453901
2315.127464	206677.552591	38.458919
2317.329505	206952.671611	38.463936
2319.998378	207181.827401	38.468954
2322.079174	207428.862319	38.473972
2324.580634	207681.201368	38.478989
2326.917460	207932.488537	38.484007
2329.170398	208178.801050	38.489024
2331.563029	208424.203790	38.494042
2333.708989	208678.761478	38.499060
2336.386824	208933.502501	38.504077
2338.750402	209198.196415	38.509095
2341.400274	209433.127244	38.514112
2343.582479	209678.530300	38.519130
2345.948918	209931.611008	38.524148
2348.390646	210173.547225	38.529165
2350.491285	210438.605515	38.534183
2352.758167	210686.868229	38.539200
2355.197046	210948.904384	38.544218
2357.408454	211201.545087	38.549236
2359.912208	211446.472470	38.554253
2362.211911	211718.207723	38.559271
2365.088738	211965.388526	38.564288
2367.135401	212223.493052	38.569306
2369.382729	212472.527578	38.574324
2371.822434	212722.573608	38.579341
2373.863192	212976.073580	38.584359
2376.515911	213192.825088	38.589376
2379.045221	213419.550328	38.594394
2380.852694	213661.282917	38.599412
2383.114676	213894.095361	38.604429
2385.198866	214120.728534	38.609447
2387.489625	214346.847293	38.614464
2389.777455	214606.776600	38.619482
2392.084515	214858.210245	38.624500
2394.295335	215097.751196	38.629517
2396.162985	215357.775409	38.634535
2398.430105	215620.009909	38.639552
2400.755572	215883.708931	38.644570
2403.294745	216155.462605	38.649588
2405.846447	216418.289876	38.654605
2408.250665	216694.472687	38.659623
2410.678949	216961.079706	38.664640
2412.897255	217255.881738	38.669658
2415.539344	217544.840935	38.674676
2418.185463	217799.710461	38.679693
2420.191203	218078.717054	38.684711
2422.775205	218357.988596	38.689728
2425.468792	218650.321457	38.694746
2428.075723	218925.579431	38.699764
2430.627726	219209.912674	38.704781
2432.924753	219503.251419	38.709799
2435.755290	219771.811334	38.714816
2437.798406	220063.237256	38.719834
2440.140713	220356.165947	38.724852
2442.781878	220628.047532	38.729869
2445.303826	220925.927245	38.734887
2447.971703	221211.151369	38.739904
2450.452026	221504.253165	38.744922
2452.799801	221792.374397	38.749940
2455.503505	222079.081706	38.754957
2458.159415	222374.025538	38.759975
2460.832859	222653.718177	38.764992
2463.433207	222931.315646	38.770010
2465.596820	223272.343711	38.775028
2468.140822	223549.977716	38.780045
2470.607125	223844.957199	38.785063
2473.108987	224126.066355	38.790080
2475.663267	224403.333509	38.795098
2478.157532	224708.584184	38.800116
2480.881710	224992.543546	38.805133
2483.176878	225286.349201	38.810151
2485.946175	225564.513228	38.815168
2488.559464	225859.476835	38.820186
2490.432106	226138.419807	38.825204
2493.642873	226420.059501	38.830221
2495.595565	226703.270908	38.835239
2498.079078	226990.462536	38.840256
2501.043103	227268.030027	38.845274
2503.427509	227561.994701	38.850292
2506.080868	227855.460638	38.855309
2508.840775	228124.885647	38.860327
2510.941447	228376.486017	38.865344
2513.045914	228636.746760	38.870362
2515.136162	228904.248591	38.875380
2517.972104	229153.017252	38.880397
2520.175385	229425.404337	38.885415
2522.421510	229688.490204	38.890432
2525.050199	229953.141636	38.895450
2527.215329	230227.340411	38.900468
2529.566720	230504.659753	38.905485
2532.082565	230783.198350	38.910503
2534.521954	231067.159538	38.915520
2537.244682	231359.508640	38.920538
2539.444170	231653.135258	38.925556
2542.120722	231945.061770	38.930573
2544.456031	232242.173584	38.935591
2546.721466	232541.583200	38.940608
2549.665078	232836.797262	38.945626
2552.322440	233148.134437	38.950644
2554.921958	233451.049671	38.955661
2557.778074	233772.973709	38.960679
2560.250352	234060.926174	38.965696
2563.253036	234362.637446	38.970714
2565.333525	234670.540540	38.975732
2568.433285	234967.717383	38.980749
2570.911575	235289.960205	38.985767
2573.410049	235589.189827	38.990784
2576.139014	235891.457033	38.995802
2578.694644	236196.038468	39.000820
2581.619654	236496.193699	39.005837
2584.227502	236812.375875	39.010855
2586.726180	237116.689634	39.015872
2589.426421	237429.811158	39.020890
2592.017794	237738.099639	39.025908
2594.745659	238038.265072	39.030925
2597.487580	238347.826791	39.035943
2599.755551	238661.706142	39.040960
2602.785092	238977.218279	39.045978
2605.360873	239291.431633	39.050996
2607.890406	239606.465974	39.056013
2610.539118	239905.277430	39.061031
2612.977703	240223.350426	39.066048
2615.803039	240540.169244	39.071066
2618.254099	240853.238263	39.076084
2620.651184	241176.324176	39.081101
2623.560128	241485.410769	39.086119
2626.168251	241804.985176	39.091136
2628.911740	242123.192785	39.096154
2631.381124	242444.492653	39.101172
2634.182319	242758.527165	39.106189
2636.728931	243081.670660	39.111207
2639.143183	243402.397531	39.116224
2642.054032	243720.481116	39.121242
2644.229198	244053.744444	39.126260
2647.143724	244365.809156	39.131277
2649.729614	244685.445215	39.136295
2652.134109	244975.722360	39.141312
2654.693885	245267.601177	39.146330
2657.037468	245560.962711	39.151348
2659.736110	245864.403512	39.156365
2662.048611	246161.886172	39.161383
2664.202438	246463.026921	39.166400
2667.190130	246782.401053	39.171418
2669.160099	247101.048085	39.176436
2671.714267	247418.815854	39.181453
2674.723633	247741.236808	39.186471
2676.923197	248080.272054	39.191488
2679.791464	248416.687436	39.196506
2682.705209	248754.290224	39.201524
2685.072369	249090.837283	39.206541
2687.701095	249430.493407	39.211559
2689.985349	249779.679545	39.216576
2693.100176	250121.089064	39.221594
2695.943990	250479.485026	39.226612
2698.845223	250835.357930	39.231629
2701.763265	251183.989486	39.236647
2704.585466	251536.675809	39.241664
2707.635250	251875.914723	39.246682
2709.910067	252234.328360	39.251700
2712.970086	252577.631303	39.256717
2715.673687	252938.493234	39.261735
2718.209290	253288.942315	39.266752
2721.391192	253639.162693	39.271770
2723.964173	254001.292098	39.276788
2726.652144	254359.314255	39.281805
2729.284574	254711.554198	39.286823
2731.790408	255089.394771	39.291840
2734.974302	255434.613880	39.296858
2737.389223	255808.456657	39.301876
2740.502057	256176.524870	39.306893
2743.103578	256544.776316	39.311911
2746.015198	256910.312033	39.316928
2749.099413	257267.666858	39.321946
2751.630605	257635.829665	39.326964
2754.605188	258009.435184	39.331981
2757.788048	258365.836218	39.336999
2760.446828	258734.793439	39.342016
2763.297863	259085.176881	39.347034
2766.116301	259453.779664	39.352052
2768.748128	259808.187044	39.357069
2771.721068	260166.757736	39.362087
2774.615997	260539.820822	39.367104
2777.637101	260890.662424	39.372122
2780.335700	261254.333145	39.377140
2782.666751	261605.869177	39.382157
2786.004030	261965.146574	39.387175
2788.476578	262325.729870	39.392192
2791.456249	262679.806344	39.397210
2794.285091	263041.731203	39.402228
2797.462256	263400.756173	39.407245
2799.918797	263744.653842	39.412263
2802.376541	264075.545316	39.417280
2805.153180	264393.710481	39.422298
2807.520451	264731.729733	39.427316
2810.102222	265056.327895	39.432333
2812.630318	265381.011037	39.437351
2815.121636	265737.098529	39.442368
2818.064415	266066.695565	39.447386
2820.526012	266436.074196	39.452404
2823.291037	266781.195847	39.457421
2826.121433	267131.210221	39.462439
2828.644004	267506.041733	39.467456
2831.883361	267867.855177	39.472474
2834.186948	268237.438015	39.477492
2836.871114	268612.930605	39.482509
2840.128310	268996.207723	39.487527
2842.526765	269376.826682	39.492544
2846.021112	269758.898153	39.497562
2848.377155	270136.374236	39.502580
2851.079452	270521.772334	39.507597
2853.923587	270912.609878	39.512615
2856.834383	271322.057708	39.517632
2860.089198	271714.100736	39.522650
2862.936508	272108.570942	39.527668
2865.764848	272509.979408	39.532685
2868.611178	272914.890813	39.537703
2871.216103	273313.311867	39.542720
2874.432153	273716.462900	39.547738
2877.607019	274132.068198	39.552756
2880.582095	274528.195362	39.557773
2883.706685	274928.211019	39.562791
2886.680129	275338.920065	39.567808
2889.558371	275738.136442	39.572826
2892.388784	276149.833460	39.577844
2895.093083	276548.035800	39.582861
2898.325596	276959.084813	39.587879
2901.107018	277364.565623	39.592896
2904.172313	277779.451484	39.597914
2907.144799	278187.340605	39.602932
2910.222359	278582.612901	39.607949
2913.353660	278995.481116	39.612967
2915.737172	279419.670453	39.617984
2918.964966	279819.262525	39.623002
2922.224843	280231.093764	39.628020
2925.227293	280637.427632	39.633037
2928.130420	281040.347568	39.638055
2930.968020	281450.619212	39.643072
2934.074855	281856.885078	39.648090
2937.082876	282265.223995	39.653108
2939.568896	282670.038005	39.658125
2942.569641	283073.322263	39.663143
2945.775358	283488.614899	39.668160
2948.959718	283896.315023	39.673178
2951.680265	284304.316852	39.678196
2954.700098	284723.575351	39.683213
2957.520540	285120.053006	39.688231
2960.302614	285495.858236	39.693248
2963.057506	285862.217477	39.698266
2965.992055	286246.406289	39.703284
2968.422065	286623.612532	39.708301
2971.434424	287000.319762	39.713319
2974.484931	287390.103088	39.718336
2976.984370	287773.216012	39.723354
2980.097260	288173.276753	39.728372
2982.625751	288574.547223	39.733389
2985.782161	288974.015800	39.738407
2988.471677	289393.295737	39.743424
2991.393681	289791.123736	39.748442
2994.413768	290209.562683	39.753460
2997.220187	290635.528614	39.758477
3000.350086	291046.277285	39.763495
3002.811590	291479.510811	39.768512
3005.877433	291918.617556	39.773530
3009.115610	292356.070489	39.778548
3011.986141	292795.028760	39.783565
3015.247944	293243.907445	39.788583
3018.266729	293685.863462	39.793600
3021.220457	294126.889018	39.798618
3024.289687	294578.462756	39.803636
3027.305205	295027.580025	39.808653
3030.846665	295475.622406	39.813671
3033.628454	295925.739995	39.818688
3037.148569	296386.967430	39.823706
3040.335366	296827.670911	39.828724
3043.053839	297295.094122	39.833741
3046.081048	297744.101754	39.838759
3049.329285	298209.863903	39.843776
3052.470338	298665.201691	39.848794
3055.619882	299106.540634	39.853812
3058.340715	299581.552623	39.858829
3062.178202	300025.447498	39.863847
3065.098480	300493.033497	39.868864
3068.574852	300937.262478	39.873882
3071.496890	301393.008547	39.878900
3074.362968	301858.440028	39.883917
3077.939142	302305.392694	39.888935
3080.912602	302763.158685	39.893952
3084.244703	303217.920006	39.898970
3087.256210	303672.171832	39.903988
3090.509406	304125.139346	39.909005
3093.677772	304573.876913	39.914023
3096.350283	305035.620462	39.919040
3099.464919	305495.158855	39.924058
3102.492477	305950.721592	39.929076
3105.506048	306409.409247	39.934093
3108.803501	306864.367337	39.939111
3111.897504	307340.590642	39.944128
3115.077857	307797.062588	39.949146
3118.161687	308253.827558	39.954164
3120.815061	308719.040954	39.959181
3124.143852	309172.893573	39.964199
3127.264953	309602.368159	39.969216
3130.046690	310041.419783	39.974234
3133.211748	310462.197611	39.979252
3135.893684	310894.657938	39.984269
3139.093515	311322.539004	39.989287
3141.753097	311758.961911	39.994304
3144.690234	312213.245657	39.999322
3147.977046	312655.153653	40.004340
3150.304462	313124.210802	40.009357
3154.050456	313563.553367	40.014375
3156.752346	314053.628304	40.019392
3159.852266	314517.045595	40.024410
3163.309368	314981.242474	40.029428
3166.235829	315461.877813	40.034445
3169.254684	315937.467404	40.039463
3172.318064	316439.157050	40.044480
3175.691708	316911.155542	40.049498
3179.159413	317408.865007	40.054516
3182.154203	317901.948147	40.059533
3185.487049	318396.016583	40.064551
3188.325382	318898.694258	40.069568
3191.577247	319400.922862	40.074586
3194.859341	319911.423476	40.079604
3198.311825	320414.808500	40.084621
3201.605348	320927.079425	40.089639
3205.131769	321439.793124	40.094656
3208.108974	321948.552669	40.099674
3211.464451	322453.922479	40.104692
3214.618011	322968.616369	40.109709
3218.542144	323475.312444	40.114727
3221.627675	323987.318956	40.119744
3224.882219	324497.467108	40.124762
3228.594336	325001.495557	40.129780
3231.681848	325519.663499	40.134797
3235.521634	326015.031009	40.139815
3238.446547	326526.945557	40.144832
3242.088376	327030.769352	40.149850
3245.346015	327523.857843	40.154868
3248.453863	328031.924471	40.159885
3252.087030	328530.483265	40.164903
3255.356549	329036.714691	40.169920
3258.370528	329537.396422	40.174938
3261.950091	330046.060708	40.179956
3265.104075	330546.358048	40.184973
3268.650264	331041.231881	40.189991
3271.848401	331557.107168	40.195008
3275.048733	332056.599677	40.200026
3278.663404	332537.892395	40.205044
3281.525184	333051.600971	40.210061
3285.012736	333545.628914	40.215079
3288.470520	334035.315931	40.220096
3291.865271	334556.623199	40.225114
3295.071134	335044.743199	40.230132
3298.346633	335541.101164	40.235149
3301.392737	336022.307366	40.240167
3304.331303	336500.200809	40.245184
3307.632708	336962.696899	40.250202
3310.968818	337417.312921	40.255220
3313.608897	337885.721785	40.260237
3317.048468	338359.612284	40.265255
3319.911280	338822.875566	40.270272
3323.039398	339299.906114	40.275290
3326.333837	339795.670401	40.280308
3329.486056	340284.775644	40.285325
3332.580418	340775.638153	40.290343
3335.905414	341270.065699	40.295360
3339.199077	341767.515633	40.300378
3342.304951	342264.534228	40.305396
3345.643840	342796.701507	40.310413
3348.744210	343314.861667	40.315431
3351.965645	343836.222599	40.320448
3355.317162	344369.744947	40.325466
3358.714433	344906.301856	40.330484
3362.295523	345441.453832	40.335501
3365.766216	345978.217788	40.340519
3369.041751	346521.278382	40.345536
3372.344696	347068.163006	40.350554
3376.163465	347598.662219	40.355572
3379.399348	348161.388525	40.360589
3382.798907	348702.377663	40.365607
3386.252710	349251.146609	40.370624
3389.778093	349819.750799	40.375642
3393.139814	350368.243916	40.380660
3396.572177	350930.453990	40.385677
3400.495547	351476.333904	40.390695
3403.796781	352028.957542	40.395712
3407.354827	352594.684213	40.400730
3411.246710	353132.860491	40.405748
3414.602964	353687.996542	40.410765
3417.934819	354241.912099	40.415783
3421.892993	354803.287074	40.420800
3425.297617	355354.056962	40.425818
3429.125902	355893.915262	40.430836
3432.543276	356438.858609	40.435853
3435.862287	356985.309187	40.440871
3439.499064	357529.266835	40.445888
3442.692602	358078.212739	40.450906
3446.552560	358623.036834	40.455924
3450.084280	359184.607854	40.460941
3453.566828	359719.022169	40.465959
3457.196329	360255.920066	40.470976
3460.236497	360810.417844	40.475994
3463.648713	361358.175306	40.481012
3466.903900	361904.529977	40.486029
3470.436876	362453.753080	40.491047
3473.981378	363010.175711	40.496064
3477.252601	363566.584131	40.501082
3481.013028	364106.031519	40.506100
3484.415712	364669.714974	40.511117
3487.471342	365205.032857	40.516122
3491.391709	365707.626856	40.521127
3493.887351	366168.867123	40.526132
3497.248753	366556.258983	40.531136
3499.926350	366912.792338	40.536141
3502.335578	367208.355126	40.541146
3504.694220	367463.394913	40.546151
3506.640365	367680.412021	40.551156
3508.687934	367833.934911	40.556160
3509.761217	367956.597882	40.561165
3511.303274	368039.675576	40.566170
3512.678819	368112.221176	40.571175
3513.790835	368129.600123	40.576180
3514.386186	368124.875682	40.581184
3515.003414	368102.135138	40.586189
3515.705406	368056.865356	40.591194
3515.948494	367997.140885	40.596199
3515.892383	367919.883419	40.601204
3516.571599	367825.921561	40.606208
3516.748844	367741.783064	40.611213
3516.800530	367630.416023	40.616218
3517.080626	367498.862584	40.621223
3517.290331	367374.367319	40.626228
3517.344542	367249.718190	40.631232
3516.948561	367114.428727	40.636237
3517.077565	366970.380060	40.641242
3516.668337	366832.471281	40.646247
3516.439600	366700.334412	40.651252
3516.587103	366546.537014	40.656256
3516.143165	366410.795031	40.661261
3515.794057	366258.703469	40.666266
3515.668528	366112.020795	40.671271
3514.913735	365972.637429	40.676276
3515.009564	365835.358143	40.681280
3514.855709	365703.231944	40.686285
3514.786743	365569.183712	40.691290
3514.774095	365432.378324	40.696295
3514.232056	365300.312310	40.701300
3514.215900	365157.476611	40.706304
3513.833488	365038.208007	40.711309
3513.285821	364921.611328	40.716314
3513.331252	364799.552023	40.721319
3513.002267	364680.019601	40.726324
3513.165474	364547.178388	40.731328
3512.369213	364438.507289	40.736333
3512.487434	364322.770679	40.741338
3512.111331	364204.669313	40.746343
3511.593435	364106.639819	40.751348
3511.568619	363998.990705	40.756352
3511.380203	363906.633582	40.761357
3510.909248	363813.125068	40.766362
3510.616506	363720.631399	40.771367
3510.451934	363629.338603	40.776372
3510.584693	363536.955413	40.781376
3510.300479	363457.385506	40.786381
3510.212939	363372.288412	40.791386
3510.068511	363288.294261	40.796391
3509.718343	363217.894317	40.801396
3509.914913	363135.347200	40.806400
3509.763311	363062.854637	40.811405
3509.341749	362987.173188	40.816410
3509.397811	362913.299008	40.821415
3508.834217	362845.451245	40.826420
3508.826055	362780.645265	40.831424
3508.319375	362732.456998	40.836429
3508.701524	362656.775187	40.841434
3508.521895	362601.537806	40.846439
3508.324722	362547.041031	40.851444
3508.621071	362487.275449	40.856448
3508.288258	362429.034156	40.861453
3508.268445	362375.577824	40.866458
3507.942841	362333.518164	40.871463
3507.679374	362281.143479	40.876468
3507.828491	362216.286411	40.881472
3507.541836	362173.202655	40.886477
3507.408497	362136.074182	40.891482
3507.677324	362080.816187	40.896487
3507.622133	362043.777069	40.901492
3507.472546	361990.926048	40.906496
3507.379992	361954.401666	40.911501
3507.115398	361898.693434	40.916506
3507.215281	361865.573646	40.921511
3506.801333	361845.181271	40.926516
3506.913894	361787.810247	40.931520
3506.537614	361760.770704	40.936525
3506.856908	361731.153011	40.941530
3506.999945	361683.700651	40.946535
3506.745383	361642.417944	40.951540
3506.944112	361612.692010	40.956544
3506.665044	361583.957614	40.961549
3506.487974	361549.431007	40.966554
3506.576101	361514.582554	40.971559
3506.438104	361485.774908	40.976564
3506.687148	361451.664330	40.981568
3506.351090	361416.628407	40.986573
3506.145911	361390.655754	40.991578
3506.078477	361372.167689	40.996583
3506.164691	361342.739270	41.001588
3506.267797	361318.600801	41.006592
3505.963789	361303.076324	41.011597
3506.056762	361267.819798	41.016602
3506.180708	361245.510066	41.021607
3505.763353	361217.051762	41.026612
3506.212625	361190.924654	41.031616
3505.792133	361174.782413	41.036621
3506.085461	361148.578151	41.041626
3506.314107	361116.378967	41.046631
3505.861697	361097.544524	41.051636
3505.921059	361069.723247	41.056640
3505.632527	361049.030803	41.061645
3505.759988	361023.285266	41.066650
3505.901581	361010.794609	41.071655
3505.527741	360988.258099	41.076660
3505.830258	360961.365252	41.081664
3505.658797	360937.880686	41.086669
3505.459441	360928.929948	41.091674
3505.485803	360912.029949	41.096679
3505.771992	360904.834534	41.101684
3505.566909	360874.306822	41.106688
3505.437058	360863.411217	41.111693
3505.646439	360844.014038	41.116698
3505.754156	360822.342814	41.121703
3505.707048	360810.874313	41.126708
3505.755151	360781.833257	41.131712
3505.638322	360753.098158	41.136717
3505.434339	360752.417962	41.141722
3505.249071	360730.945685	41.146727
3505.605049	360718.853638	41.151732
3505.548651	360708.226289	41.156736
3505.676165	360687.442474	41.161741
3505.439838	360672.110658	41.166746
3505.256134	360636.922848	41.171751
3505.182913	360631.616301	41.176756
3505.209781	360616.471873	41.181760
3505.290606	360592.056655	41.186765
3504.904356	360588.326332	41.191770
3505.268910	360561.347116	41.196775
3505.359412	360560.086003	41.201780
3505.567627	360554.429608	41.206784
3505.352474	360527.185772	41.211789
3505.173545	360516.908546	41.216794
3505.138441	360501.748432	41.221799
3505.292553	360491.087758	41.226804
3505.106389	360482.949117	41.231808
3505.039285	360467.743159	41.236813
3504.971564	360461.036203	41.241818
3505.194818	360447.718223	41.246823
3505.149710	360433.221261	41.251828
3505.037689	360421.152228	41.256832
3505.042824	360408.682985	41.261837
3505.310071	360391.108576	41.266842
3505.745548	360380.835979	41.271847
3505.095197	360364.424449	41.276852
3505.370329	360350.029514	41.281856
3505.246326	360327.122402	41.286861
3505.163868	360313.750928	41.291866
3505.128435	360311.695447	41.296871
3505.130074	360299.481187	41.301876
3505.168305	360284.767439	41.306880
3505.016607	360273.569802	41.311885
3505.403493	360254.984040	41.316890
3505.090989	360235.949019	41.321895
3505.064895	360227.937706	41.326900
3504.821851	360214.591590	41.331904
3504.689867	360204.408660	41.336909
3504.792771	360196.962207	41.341914
3505.021733	360186.340525	41.346919
3504.760897	360181.674289	41.351924
3505.199189	360173.436881	41.356928
3504.763744	360154.115911	41.361933
3505.146193	360147.923005	41.366938
3505.276130	360131.031804	41.371943
3504.902837	360120.276297	41.376948
3504.994971	360113.391346	41.381952
3504.981504	360103.265997	41.386957
3505.284708	360091.716502	41.391962
3504.900221	360074.601248	41.396967
3504.736902	360067.145968	41.401972
3505.041911	360054.120307	41.406976
3505.013741	360053.666768	41.411981
3504.878755	360033.534871	41.416986
3504.912448	360018.134716	41.421991
3504.884591	360023.508275	41.426996
3505.117693	359997.160229	41.432000
3504.894769	359997.449966	41.437005
3505.228916	359973.681433	41.442010
3505.537826	359967.983606	41.447015
3504.914916	359954.748359	41.452020
3505.418138	359930.698616	41.457024
3505.085561	359920.649120	41.462029
3505.016060	359908.446006	41.467034
3505.320428	359880.636201	41.472039
3505.011031	359870.761153	41.477044
3504.743851	359858.691061	41.482048
3505.049308	359851.288873	41.487053
3504.734323	359849.252118	41.492058
3504.931423	359829.551117	41.497063
3504.470235	359832.219567	41.502068
3504.913037	359793.827670	41.507072
3504.579624	359798.282602	41.512077
3504.682285	359800.658352	41.517082
3504.923359	359776.726311	41.522087
3505.047855	359786.986928	41.527092
3505.025755	359757.167519	41.532096
3504.841140	359759.919484	41.537101
3504.805809	359743.843104	41.542106
3504.704059	359723.146007	41.547111
3504.829746	359729.080591	41.552116
3504.720972	359711.463591	41.557120
3504.665075	359711.421572	41.562125
3504.738988	359704.412212	41.567130
3505.063184	359699.500770	41.572135
3504.779939	359696.644711	41.577140
3504.789175	359683.004105	41.582144
3504.890385	359674.972576	41.587149
3505.003968	359662.689566	41.592154
3505.252030	359652.751796	41.597159
3504.769299	359626.923847	41.602164
3505.012347	359606.935583	41.607168
3504.737999	359607.615146	41.612173
3504.879930	359602.172688	41.617178
3505.062883	359585.629163	41.622183
3504.766351	359567.609205	41.627188
3504.974945	359551.290632	41.632192
3504.946579	359553.025502	41.637197
3504.903452	359543.719006	41.642202
3504.839934	359521.819802	41.647207
3504.551492	359528.099786	41.652212
3504.888584	359504.279664	41.657216
3504.899985	359509.418058	41.662221
3504.699562	359498.304283	41.667226
3504.908832	359469.618654	41.672231
3504.881234	359470.819032	41.677236
3504.798656	359460.780812	41.682240
3504.748118	359452.620557	41.687245
3505.049638	359430.383697	41.692250
3504.754427	359414.144719	41.697255
3504.552768	359409.316375	41.702260
3504.764574	359403.888296	41.707264
3504.555018	359387.075948	41.712269
3504.685337	359389.141988	41.717274
3504.870111	359384.965053	41.722279
3504.579373	359363.839643	41.727284
3504.686572	359358.708006	41.732288
3504.435093	359372.641535	41.737293
3504.681192	359356.851342	41.742298
3504.634885	359339.758707	41.747303
3504.594224	359351.928559	41.752308
3504.721789	359325.393259	41.757312
3504.726988	359313.458098	41.762317
3504.502789	359318.201166	41.767322
3505.100285	359306.986659	41.772327
3504.816778	359284.358731	41.777332
3505.179773	359286.209869	41.782336
3504.676025	359279.622569	41.787341
3504.575893	359282.946473	41.792346
3504.459864	359270.648768	41.797351
3504.131082	359252.964595	41.802356
3504.606624	359245.637215	41.807360
3504.356184	359236.567004	41.812365
3504.455388	359243.549139	41.817370
3504.638248	359236.598829	41.822375
3504.714878	359228.622004	41.827380
3504.816645	359216.595214	41.832384
3504.687857	359209.134343	41.837389
3504.659774	359199.723617	41.842394
3505.162373	359184.808895	41.847399
3504.774500	359191.104639	41.852404
3504.768670	359167.516688	41.857408
3504.841466	359171.652998	41.862413
3504.489541	359144.913486	41.867418
3504.654277	359130.128496	41.872423
3504.460888	359141.762720	41.877428
3504.686584	359112.768926	41.882432
3504.394470	359112.637014	41.887437
3504.585527	359112.174258	41.892442
3504.740651	359101.869369	41.897447
3504.710681	359090.906682	41.902452
3504.637535	359084.225838	41.907456
3504.715928	359071.057612	41.912461
3504.839564	359061.190284	41.917466
3504.629818	359059.162306	41.922471
3504.969155	359046.436308	41.927476
3504.832096	359030.706579	41.932480
3504.635176	359029.414523	41.937485
3504.583865	359006.037256	41.942490
3504.797600	359000.837846	41.947495
3504.793745	358994.425949	41.952500
3504.732211	358980.236508	41.957504
3504.951350	358975.672407	41.962509
3504.542331	358962.326735	41.967514
3504.643977	358953.633407	41.972519
3504.332745	358947.804473	41.977524
3504.397536	358943.900934	41.982528
3504.529420	358924.057195	41.987533
3504.370678	358916.601014	41.992538
3504.932033	358904.679622	41.997543
3504.360231	358932.506888	42.002548
3504.541022	358899.066904	42.007552
3504.492638	358887.012875	42.012557
3504.349117	358896.832562	42.017562
3504.442409	358896.385258	42.022567
3504.343216	358885.051767	42.027572
3504.828851	358859.910070	42.032576
3504.535860	358878.125343	42.037581
3504.311392	358872.562598	42.042586
3504.514372	358840.798546	42.047591
3504.362633	358852.986082	42.052596
3504.420815	358860.356457	42.057600
3504.567736	358860.587735	42.062605
3504.285054	358836.712582	42.067610
3504.571439	358829.211468	42.072615
3504.760986	358825.364538	42.077620
3504.950071	358812.764018	42.082624
3504.955570	358803.526034	42.087629
3504.572847	358795.087373	42.092634
3505.083927	358767.320596	42.097639
3504.714064	358770.280026	42.102644
3504.485626	358774.514883	42.107648
3504.509692	358744.076834	42.112653
3504.482303	358735.505651	42.117658
3504.712761	358744.044807	42.122663
3504.533043	358738.118718	42.127668
3504.526420	358716.362839	42.132672
3504.381845	358710.761999	42.137677
3504.225508	358721.092682	42.142682
3504.551862	358716.689735	42.147687
3504.470760	358696.854127	42.152692
3504.465440	358685.098602	42.157696
3504.563861	358697.679226	42.162701
3504.366495	358687.608099	42.167706
3504.524557	358662.136382	42.172711
3504.255839	358673.197350	42.177716
3504.605098	358664.973763	42.182720
3504.385382	358666.077297	42.187725
3504.469852	358655.045527	42.192730
3504.626076	358652.527084	42.197735
3504.231753	358655.363154	42.202740
3504.293134	358640.238099	42.207744
3504.115799	358625.659712	42.212749
3504.377055	358618.417007	42.217754
3504.385927	358615.412919	42.222759
3503.995061	358621.836443	42.227764
3504.414132	358623.805977	42.232768
3504.350285	358631.399251	42.237773
3504.183159	358612.696866	42.242778
3504.485710	358587.634865	42.247783
3504.527680	358595.618566	42.252788
3504.656418	358597.557656	42.257792
3504.702877	358581.722431	42.262797
3504.507451	358575.646125	42.267802
3504.585981	358569.831873	42.272807
3504.333483	358568.294122	42.277812
3504.390812	358543.550778	42.282816
3504.354452	358551.724996	42.287821
3504.074250	358554.975628	42.292826
3504.552654	358558.437148	42.297831
3504.247142	358545.202234	42.302836
3504.359649	358532.028471	42.307840
3504.115995	358529.064297	42.312845
3503.930822	358520.059976	42.317850
3504.332774	358524.017074	42.322855
3504.270814	358541.356204	42.327860
3504.667357	358526.407154	42.332864
3504.396708	358513.293954	42.337869
3504.542260	358508.665102	42.342874
3504.654113	358507.196986	42.347879
3504.542943	358503.295781	42.352884
3504.357773	358477.267502	42.357888
3504.343125	358475.234105	42.362893
3504.377261	358482.481103	42.367898
3504.711467	358481.308646	42.372903
3504.513173	358470.754131	42.377908
3504.466322	358466.461053	42.382912
3504.642744	358450.986945	42.387917
3504.281660	358452.621769	42.392922
3504.025358	358431.007020	42.397927
3504.460735	358436.002164	42.402932
3504.490219	358433.910895	42.407936
3504.384970	358430.492239	42.412941
3504.264930	358429.315247	42.417946
3504.705158	358408.684598	42.422951
3504.645536	358402.943059	42.427956
3504.597056	358420.025632	42.432960
3504.631705	358392.461191	42.437965
3504.598906	358378.852312	42.442970
3504.424081	358383.791241	42.447975
3504.205374	358385.887051	42.452980
3504.509683	358364.463568	42.457984
3504.255143	358354.045154	42.462989
3504.197899	358364.869185	42.467994
3504.201918	358355.351435	42.472999
3504.297095	358362.130757	42.478004
3504.407241	358359.466901	42.483008
3504.520362	358340.949133	42.488013
3504.089735	358329.464331	42.493018
3504.232551	358331.502995	42.498023
3504.245383	358333.842122	42.503028
3504.732458	358323.535489	42.508032
3504.530257	358306.925182	42.513037
3504.286476	358311.086163	42.518042
3504.622819	358306.045427	42.523047
3504.318257	358309.020009	42.528052
3504.557035	358284.782238	42.533056
3504.110220	358289.000763	42.538061
3504.218898	358275.954771	42.543066
3504.156315	358291.716376	42.548071
3504.413965	358283.634441	42.553076
3504.448856	358270.829135	42.558080
3504.363050	358263.793923	42.563085
3504.107002	358265.742959	42.568090
3504.470550	358252.885694	42.573095
3504.228595	358268.777449	42.578100
3504.386845	358250.583324	42.583104
3504.296960	358230.189082	42.588109
3504.111809	358233.755520	42.593114
3504.631694	358224.156196	42.598119
3504.542565	358229.717768	42.603124
3504.443668	358221.717634	42.608128
3503.926733	358214.317969	42.613133
3503.692885	358210.995968	42.618138
3503.984695	358214.181645	42.623143
3504.058788	358218.241490	42.628148
3504.335780	358217.408883	42.633152
3504.191695	358216.108452	42.638157
3503.899841	358217.477870	42.643162
3504.365947	358220.661441	42.648167
3503.990085	358203.722293	42.653172
3504.305826	358204.054123	42.658176
3504.442122	358183.827683	42.663181
3504.358541	358191.067886	42.668186
3504.608280	358186.778792	42.673191
3504.876958	358182.155892	42.678196
3504.678654	358159.641210	42.683200
3504.425082	358170.445426	42.688205
3504.437526	358151.943502	42.693210
3504.540286	358135.259482	42.698215
3504.407432	358139.631965	42.703220
3504.454931	358138.606611	42.708224
3504.474956	358126.897840	42.713229
3504.464541	358118.451102	42.718234
3504.781928	358097.381694	42.723239
3504.277300	358115.452575	42.728244
3504.231516	358100.089825	42.733248
3504.251400	358084.182300	42.738253
3504.805286	358076.638785	42.743258
3504.674000	358072.333573	42.748263
3504.445978	358068.374464	42.753268
3504.374253	358052.608646	42.758272
3504.217436	358051.691930	42.763277
3504.193196	358061.671057	42.768282
3504.424140	358053.084365	42.773287
3504.137789	358041.703924	42.778292
3504.045494	358034.415234	42.783296
3504.059263	358035.965368	42.788301
3503.967977	358029.668954	42.793306
3504.207049	358030.827212	42.798311
3503.894619	358038.790686	42.803316
3504.437272	358039.442906	42.808321
3504.411673	358037.614798	42.813325
3504.127965	358034.835056	42.818330
3504.586588	358012.801743	42.823335
3504.317065	358016.890476	42.828340
3504.502697	358010.779309	42.833345
3504.220156	358015.684408	42.838349
3504.086490	357989.774964	42.843354
3504.357826	357980.494802	42.848359
3503.969062	357986.256451	42.853364
3504.263140	357988.525688	42.858369
3504.544783	357994.512170	42.863373
3504.216608	357994.818557	42.868378
3504.325586	357976.275860	42.873383
3504.183095	357967.519162	42.878388
3504.323320	357965.919309	42.883393
3504.032732	357969.782352	42.888397
3504.106724	357973.994916	42.893402
3504.452447	357980.582002	42.898407
3504.144427	357966.736597	42.903412
3504.269956	357952.110134	42.908417
3504.079453	357941.096225	42.913421
3504.037908	357931.916408	42.918426
3504.168548	357930.343517	42.923431
3504.207260	357937.589872	42.928436
3504.271560	357945.773726	42.933441
3504.386741	357946.824335	42.938445
3504.285007	357929.256474	42.943450
3504.291165	357910.195616	42.948455
3504.053945	357913.872097	42.953460
3504.272705	357911.140153	42.958465
3504.452836	357912.104154	42.963469
3504.204945	357913.670208	42.968474
3504.449684	357894.266263	42.973479
3504.106203	357899.486373	42.978484
3504.353076	357887.563555	42.983489
3504.466376	357891.464546	42.988493
3504.199691	357888.732998	42.993498
3504.461045	357876.298945	42.998503
3504.393752	357884.071009	43.003508
3504.467753	357878.817229	43.008513
3504.416518	357872.972514	43.013517
3504.133574	357851.387169	43.018522
3504.255189	357842.690488	43.023527
3504.054517	357848.346077	43.028532
3504.123759	357840.217512	43.033537
3504.074933	357843.329826	43.038541
3504.211700	357843.817186	43.043546
3504.395450	357846.231107	43.048551
3504.484698	357843.087030	43.053556
3504.335979	357826.748026	43.058561
3504.563177	357813.123338	43.063565
3504.485385	357817.894300	43.068570
3504.597053	357808.512111	43.073575
3504.449514	357797.949428	43.078580
3504.601201	357783.395121	43.083585
3504.366541	357790.124873	43.088589
3504.241218	357776.784927	43.093594
3504.473987	357761.021776	43.098599
3504.076541	357774.266310	43.103604
3504.081002	357757.775832	43.108609
3504.378565	357761.698599	43.113613
3504.223270	357770.451587	43.118618
3504.415418	357760.140565	43.123623
3503.899935	357744.241221	43.128628
3504.108259	357739.042534	43.133633
3504.188459	357745.824308	43.138637
3504.192596	357736.128289	43.143642
3504.230815	357739.710347	43.148647
3504.295832	357744.916792	43.153652
3504.304010	357732.878986	43.158657
3504.310514	357717.075248	43.163661
3504.217170	357720.830788	43.168666
3504.250680	357710.748411	43.173671
3504.079245	357713.701984	43.178676
3504.080862	357707.823447	43.183681
3504.273565	357715.579884	43.188685
3503.985981	357709.848854	43.193690
3504.259376	357684.841898	43.198695
3504.108382	357697.793020	43.203700
3504.349289	357698.060341	43.208705
3504.225276	357699.123321	43.213709
3504.088330	357695.200679	43.218714
3504.257984	357695.021213	43.223719
3504.071046	357686.169702	43.228724
3504.352262	357672.002043	43.233729
3504.252750	357677.539871	43.238733
3504.214196	357677.062504	43.243738
3504.222295	357675.229056	43.248743
3504.304398	357678.498814	43.253748
3504.202256	357667.852585	43.258753
3504.188722	357649.634500	43.263757
3503.960933	357654.149270	43.268762
3504.161890	357648.137425	43.273767
3504.067489	357656.015599	43.278772
3504.241209	357652.196528	43.283777
3504.301105	357651.296441	43.288781
3504.085678	357655.987387	43.293786
3504.461371	357637.962242	43.298791
3504.344816	357638.438755	43.303796
3504.098485	357630.080122	43.308801
3504.520057	357628.257652	43.313805
3504.473135	357624.702483	43.318810
3504.493549	357601.058737	43.323815
3504.249905	357599.341424	43.328820
3504.348238	357588.103646	43.333825
3504.511309	357589.706533	43.338829
3504.186092	357588.053010	43.343834
3504.305160	357571.238985	43.348839
3504.180388	357576.602686	43.353844
3504.061393	357570.692305	43.358849
3504.057313	357576.596768	43.363853
3504.285442	357568.493937	43.368858
3504.355296	357574.564845	43.373863
3503.871918	357568.635723	43.378868
3504.129459	357553.784694	43.383873
3504.525710	357545.578940	43.388877
3504.216216	357541.530879	43.393882
3504.654020	357544.108232	43.398887
3504.570900	357541.194963	43.403892
3504.286257	357525.335399	43.408897
3504.368982	357511.275413	43.413901
3504.279826	357502.382965	43.418906
3504.488349	357500.034327	43.423911
3504.296442	357514.467912	43.428916
3504.468847	357491.843429	43.433921
3504.502344	357472.956213	43.438925
3504.207225	357483.054619	43.443930
3503.933405	357479.789782	43.448935
3504.321760	357481.026244	43.453940
3504.434790	357466.427060	43.458945
3504.133419	357459.527600	43.463949
3504.089039	357454.012568	43.468954
3504.374474	357449.208819	43.473959
3504.095156	357468.771162	43.478964
3503.949224	357462.076157	43.483969
3504.644411	357450.947576	43.488973
3504.235456	357438.772061	43.493978
3504.327595	357428.095068	43.498983
3504.288827	357427.312364	43.503988
3504.309668	357428.861398	43.508993
3504.238294	357434.623832	43.513997
3504.040495	357419.539375	43.519002
3504.318395	357395.269537	43.524007
3504.055572	357400.553291	43.529012
3504.246402	357393.499672	43.534017
3504.295420	357397.105494	43.539021
3504.125865	357400.364158	43.544026
3504.349401	357394.806766	43.549031
3504.329384	357378.218242	43.554036
3504.494866	357361.040545	43.559041
3504.394467	357367.291077	43.564045
3504.269046	357359.142311	43.569050
3504.315725	357364.402590	43.574055
3504.183556	357357.654500	43.579060
3504.165759	357342.745144	43.584065
3504.222705	357342.532599	43.589069
3504.122034	357333.438361	43.594074
3504.415481	357341.077141	43.599079
3504.164357	357346.282709	43.604084
3504.126840	357334.150241	43.609089
3504.037162	357315.333331	43.614093
3504.001518	357307.297602	43.619098
3504.458819	357310.584415	43.624103
3503.815282	357319.796376	43.629108
3503.973839	357305.546213	43.634113
3504.158564	357311.522651	43.639117
3504.370101	357319.734228	43.644122
3504.503187	357318.237273	43.649127
3504.474565	357304.601991	43.654132
3504.422682	357285.244699	43.659137
3504.695253	357286.066862	43.664141
3504.293856	357287.021014	43.669146
3504.428565	357262.264797	43.674151
3504.398120	357266.519378	43.679156
3504.389684	357258.224865	43.684161
3504.172788	357255.688992	43.689165
3504.128354	357261.599872	43.694170
3504.331510	357247.215405	43.699175
3503.933240	357248.474433	43.704180
3504.160608	357233.958896	43.709185
3504.034590	357233.648037	43.714189
3504.311895	357241.162147	43.719194
3504.571600	357226.183441	43.724199
3504.501876	357228.815594	43.729204
3504.330993	357198.789123	43.734209
3504.357400	357193.797270	43.739213
3504.325022	357198.459323	43.744218
3504.363372	357196.799208	43.749223
3504.380710	357191.681551	43.754228
3504.408862	357162.616049	43.759233
3504.054513	357162.875682	43.764237
3503.893010	357177.253663	43.769242
3504.462489	357163.727374	43.774247
3504.186766	357161.455271	43.779252
3504.198683	357155.727726	43.784257
3504.247240	357150.579681	43.789261
3504.062442	357142.898322	43.794266
3504.026347	357134.913532	43.799271
3503.922611	357137.398381	43.804276
3503.915108	357137.145128	43.809281
3504.148890	357134.970614	43.814285
3504.058105	357147.454305	43.819290
3504.149507	357151.129788	43.824295
3504.304528	357159.884723	43.829300
3504.562267	357137.170247	43.834305
3504.309221	357121.967196	43.839309
3504.350572	357119.543177	43.844314
3504.428717	357125.027535	43.849319
3504.096396	357117.751206	43.854324
3504.128137	357097.744432	43.859329
3504.371116	357091.089688	43.864333
3504.020684	357101.171468	43.869338
3503.862811	357087.989167	43.874343
3504.113752	357088.178563	43.879348
3504.084936	357098.158607	43.884353
3504.093171	357101.160156	43.889357
3504.240267	357091.670441	43.894362
3504.164483	357083.946392	43.899367
3504.283503	357072.247171	43.904372
3504.323444	357063.766845	43.909377
3504.362532	357077.375165	43.914381
3504.157419	357074.633839	43.919386
3504.389071	357080.730125	43.924391
3503.975943	357057.230998	43.929396
3504.056347	357041.644391	43.934401
3504.362823	357038.364134	43.939405
3504.151586	357032.926327	43.944410
3504.419041	357021.330867	43.949415
3504.037720	357034.725734	43.954420
3504.268485	357041.534698	43.959425
3504.386389	357032.787566	43.964429
3504.241807	357009.551336	43.969434
3504.254729	357005.452263	43.974439
3504.187763	357000.755075	43.979444
3504.084669	357012.350078	43.984449
3504.313195	357020.660809	43.989453
3504.462571	357016.540165	43.994458
3504.358591	356982.838532	43.999463
3503.911339	356980.160926	44.004468
3504.228735	356976.090061	44.009473
3504.238103	356965.400607	44.014477
3504.150750	356966.381463	44.019482
3504.315785	356973.200827	44.024487
3504.137983	356964.373191	44.029492
3504.376010	356953.876617	44.034497
3504.278718	356944.705430	44.039501
3504.039024	356947.720734	44.044506
3504.498144	356941.947918	44.049511
3504.295911	356952.489805	44.054516
3504.480107	356930.906558	44.059521
3504.499326	356912.224968	44.064525
3504.165839	356918.690536	44.069530
3504.362846	356911.101471	44.074535
3504.329311	356914.364111	44.079540
3503.996320	356889.198139	44.084545
3504.180098	356892.197398	44.089549
3504.289833	356893.935978	44.094554
3504.368174	356878.324199	44.099559
3504.278385	356882.995357	44.104564
3504.073024	356879.999582	44.109569
3504.186268	356863.186240	44.114573
3503.758953	356854.881533	44.119578
3504.246480	356851.445405	44.124583
3504.117366	356862.128439	44.129588
3504.460235	356853.498400	44.134593
3504.170256	356864.003281	44.139597
3504.210902	356865.167487	44.144602
3504.298111	356852.506231	44.149607
3504.125286	356838.028395	44.154612
3503.980898	356832.147387	44.159617
3504.155262	356839.957756	44.164621
3503.991442	356833.265494	44.169626
3504.109440	356838.870822	44.174631
3503.911491	356842.922889	44.179636
3503.981947	356832.325540	44.184641
3504.090565	356837.016233	44.189645
3504.001605	356853.036941	44.194650
3504.380183	356841.983723	44.199655
3504.086001	356821.672093	44.204660
3504.131412	356813.725262	44.209665
3504.314758	356816.750042	44.214669
3503.969026	356812.147799	44.219674
3504.102025	356805.739433	44.224679
3503.867838	356814.276030	44.229684
3504.190990	356807.786708	44.234689
3504.207688	356809.310969	44.239693
3503.815827	356818.508684	44.244698
3504.336943	356797.584655	44.249703
3503.898183	356802.209195	44.254708
3504.075570	356797.244331	44.259713
3503.998075	356797.154828	44.264717
3504.104778	356804.746868	44.269722
3504.379915	356794.117155	44.274727
3504.245722	356808.083761	44.279732
3504.164774	356793.056986	44.284737
3504.314344	356781.709136	44.289741
3503.905844	356777.040469	44.294746
3504.167233	356761.399717	44.299751
3503.977165	356761.073532	44.304756
3504.142496	356765.551684	44.309761
3504.076436	356767.674327	44.314765
3503.998176	356775.677327	44.319770
3504.213519	356765.515120	44.324775
3503.943287	356776.983912	44.329780
3504.156570	356782.548736	44.334785
3504.352272	356762.439566	44.339789
3504.173475	356753.230334	44.344794
3504.523116	356750.095921	44.349799
3504.247479	356742.021696	44.354804
3504.345852	356745.848793	44.359809
3504.130119	356722.012931	44.364813
3503.906006	356705.201970	44.369818
3504.153402	356708.242079	44.374823
3503.811194	356709.644945	44.379828
3504.019972	356706.278319	44.384833
3504.221598	356702.403868	44.389837
3504.014447	356706.533744	44.394842
3504.086830	356704.359277	44.399847
3504.243351	356712.732337	44.404852
3503.977445	356708.193809	44.409857
3504.280647	356714.915024	44.414861
3504.091914	356692.398164	44.419866
3504.354316	356687.827014	44.424871
3504.138185	356693.586969	44.429876
3504.221333	356678.254293	44.434881
3504.134599	356692.162533	44.439885
3503.935163	356697.207310	44.444890
3504.483267	356687.705022	44.449895
3504.181429	356670.168350	44.454900
3503.697436	356662.025258	44.459905
3503.871777	356649.070251	44.464909
3503.641965	356657.911557	44.469914
3504.229947	356660.465216	44.474919
3504.166013	356660.628047	44.479924
3504.170768	356650.626345	44.484929
3504.599983	356661.170265	44.489933
3504.272176	356661.552944	44.494938
3504.388367	356649.726832	44.499943
3504.004957	356632.253937	44.504948
3504.026826	356629.094988	44.509953
3504.094531	356632.748807	44.514957
3504.103695	356633.714413	44.519962
3504.401963	356630.893487	44.524967
3504.082635	356646.161795	44.529972
3504.232832	356627.561185	44.534977
3504.328880	356611.590255	44.539981
3503.960996	356610.299712	44.544986
3504.427476	356592.743348	44.549991
3504.376490	356603.541326	44.554996
3504.132058	356594.825948	44.560001
3504.014302	356612.250916	44.565005
3503.868262	356604.461556	44.570010
3504.013846	356589.068087	44.575015
3503.786865	356594.880664	44.580020
3503.868885	356584.408674	44.585025
3504.185607	356576.317126	44.590029
3504.016468	356571.381570	44.595034
3504.178647	356574.333368	44.600039
3504.193670	356580.285825	44.605044
3504.168171	356583.979830	44.610049
3504.383034	356570.763918	44.615053
3504.245472	356569.665996	44.620058
3504.117972	356553.323220	44.625063
3503.987609	356550.773631	44.630068
3504.128790	356547.723055	44.635073
3504.109885	356542.687404	44.640077
3504.054317	356551.602976	44.645082
3504.289117	356543.473476	44.650087
3504.569095	356543.785524	44.655092
3504.198662	356537.533049	44.660097
3504.141738	356531.485493	44.665101
3504.111307	356519.962456	44.670106
3504.173294	356506.439872	44.675111
3504.097404	356515.893068	44.680116
3504.171344	356525.856982	44.685121
3504.563963	356509.915480	44.690125
3504.429004	356502.353384	44.695130
3504.100009	356487.518416	44.700135
3503.866827	356476.256451	44.705140
3504.230786	356487.981326	44.710145
3503.948517	356484.285145	44.715149
3504.021019	356484.451855	44.720154
3504.436832	356482.528464	44.725159
3503.808586	356495.046384	44.730164
3504.183040	356491.500867	44.735169
3503.914624	356475.638403	44.740173
3503.896242	356466.658239	44.745178
3504.072391	356465.459826	44.750183
3504.038911	356468.009945	44.755188
3503.936354	356468.077090	44.760193
3503.841029	356466.641666	44.765197
3503.659432	356471.759990	44.770202
3504.072604	356458.080085	44.775207
3503.770538	356472.404145	44.780212
3504.048267	356472.971028	44.785217
3504.014939	356477.811433	44.790221
3504.318945	356478.272370	44.795226
3504.334732	356471.093605	44.800231
3504.017945	356476.207851	44.805236
3504.318538	356455.369436	44.810241
3504.252263	356446.473182	44.815245
3504.121718	356443.567346	44.820250
3504.332427	356434.754544	44.825255
3504.083848	356443.039000	44.830260
3503.979928	356440.128955	44.835265
3504.230318	356448.716252	44.840269
3504.084392	356433.190682	44.845274
3504.080267	356432.860548	44.850279
3503.928087	356414.205868	44.855284
3504.493754	356403.301114	44.860289
3504.663537	356411.748472	44.865293
3503.957659	356422.141056	44.870298
3504.476121	356407.757400	44.875303
3504.036417	356395.535595	44.880308
3503.611879	356382.395263	44.885313
3503.521247	356388.975196	44.890317
3503.937105	356376.898065	44.895322
3504.182775	356376.248515	44.900327
3504.065270	356401.486034	44.905332
3504.336259	356393.986988	44.910337
3504.000340	356398.468068	44.915341
3503.909467	356392.807581	44.920346
3504.152377	356391.929437	44.925351
3504.504841	356408.465808	44.930356
3503.774331	356400.717914	44.935361
3503.785633	356392.140210	44.940365
3503.982515	356399.234545	44.945370
3504.144440	356372.946711	44.950375
3503.945333	356370.560668	44.955380
3504.398613	356361.658611	44.960385
3504.515558	356360.036941	44.965389
3504.039552	356359.959537	44.970394
3504.194771	356352.656922	44.975399
3504.183307	356365.968050	44.980404
3503.903398	356357.436376	44.985409
3504.116535	356338.011375	44.990413
3503.992870	356328.462525	44.995418
3504.083444	356323.307754	45.000423
3504.028732	356339.119628	45.005428
3504.359300	356339.041960	45.010433
3504.355218	356331.713628	45.015437
3504.236644	356344.074672	45.020442
3504.320286	356332.406319	45.025447
3503.902420	356319.239468	45.030452
3504.027168	356309.575002	45.035457
3504.158176	356296.728546	45.040461
3504.168057	356305.430231	45.045466
3504.344223	356304.206365	45.050471
3504.014353	356312.758173	45.055476
3504.233499	356303.765878	45.060481
3504.383178	356301.706415	45.065485
3503.923146	356283.100352	45.070490
3504.099715	356281.265669	45.075495
3504.600345	356271.210952	45.080500
3504.090996	356264.929507	45.085505
3504.114512	356269.989979	45.090509
3503.941062	356273.478362	45.095514
3504.449902	356262.328081	45.100519
3504.052971	356257.148577	45.105524
3504.036046	356246.590366	45.110529
3504.292080	356238.432013	45.115533
3504.055466	356249.386651	45.120538
3503.819205	356232.704692	45.125543
3503.911736	356244.752460	45.130548
3504.072944	356237.830601	45.135553
3504.030475	356248.958133	45.140557
3503.916704	356251.520956	45.145562
3504.172470	356257.002778	45.150567
3503.896701	356259.845689	45.155572
3504.145589	356247.387754	45.160577
3504.178887	356223.130568	45.165581
3503.848680	356229.672050	45.170586
3504.005843	356220.053338	45.175591
3503.948875	356215.965249	45.180596
3504.009245	356216.235671	45.185601
3503.954772	356220.341451	45.190605
3503.644446	356216.929613	45.195610
3503.885170	356208.646435	45.200615
3504.052908	356222.081961	45.205620
3503.949304	356227.518804	45.210625
3504.328936	356218.017613	45.215629
3503.938576	356229.352831	45.220634
3504.006612	356230.614514	45.225639
3503.932647	356230.219075	45.230644
3504.069861	356225.616777	45.235649
3504.234562	356221.595439	45.240653
3503.709765	356208.470911	45.245658
3504.061066	356192.103224	45.250663
3503.885603	356203.684406	45.255668
3503.919584	356195.408460	45.260673
3504.403459	356193.092578	45.265677
3504.129269	356196.062484	45.270682
3504.100817	356203.599636	45.275687
3503.951278	356207.415069	45.280692
3504.105503	356194.055956	45.285697
3504.260518	356200.927906	45.290701
3504.109964	356191.154249	45.295706
3504.100816	356177.006621	45.300711
3503.968177	356179.165261	45.305716
3504.418275	356168.151486	45.310721
3504.490641	356174.196718	45.315725
3504.198417	356179.281663	45.320730
3504.009278	356160.530939	45.325735
3504.230264	356158.205718	45.330740
3504.480981	356137.934913	45.335745
3504.465655	356140.711212	45.340749
3504.057415	356134.388320	45.345754
3504.908845	356143.669545	45.350759
3504.796781	356120.325971	45.355764
3504.121651	356104.298652	45.360769
3504.467359	356104.600312	45.365773
3504.207258	356103.241822	45.370778
3504.396100	356070.205833	45.375783
3504.070419	356068.628675	45.380788
3504.085265	356062.875094	45.385793
3504.246080	356062.849709	45.390797
3504.070605	356076.339530	45.395802
3504.345560	356057.159130	45.400807
3504.290005	356055.971888	45.405812
3504.124779	356042.586890	45.410817
3504.011969	356032.349170	45.415821
3504.050354	356033.157478	45.420826
3504.091760	356021.826556	45.425831
3504.087847	356024.957331	45.430836
3504.245809	356026.103010	45.435841
3504.545795	356030.763527	45.440845
3504.135949	356028.767056	45.445850
3504.116483	356011.974408	45.450855
3503.967039	356003.040327	45.455860
3504.071725	356000.453554	45.460865
3504.050093	356008.371379	45.465869
3504.188239	356011.810523	45.470874
3504.142933	356002.656395	45.475879
3503.843179	356017.260147	45.480884
3504.165925	356014.537111	45.485889
3504.380941	356006.130723	45.490893
3503.753065	355996.661517	45.495898
3503.948479	355982.659634	45.500903
3504.107262	355966.805823	45.505908
3504.165066	355978.528319	45.510913
3504.268592	355975.178283	45.515917
3504.148105	355976.571566	45.520922
3504.172761	355974.862680	45.525927
3504.146898	355983.519174	45.530932
3504.074672	355962.841285	45.535937
3504.337013	355946.385789	45.540941
3503.923994	355951.718886	45.545946
3503.927379	355942.531601	45.550951
3503.920392	355942.125572	45.555956
3504.027370	355934.805074	45.560961
3504.384885	355941.797737	45.565965
3504.119429	355947.921848	45.570970
3504.055181	355950.451409	45.575975
3503.626250	355950.900974	45.580980
3504.088986	355946.578018	45.585985
3504.066773	355951.594854	45.590989
3503.940785	355941.155613	45.595994
3503.965542	355922.905400	45.600999
3503.904857	355914.364443	45.606004
3503.878554	355905.410879	45.611009
3503.794492	355917.792019	45.616013
3503.774723	355917.846077	45.621018
3503.688387	355926.741174	45.626023
3503.519024	355923.408826	45.631028
3503.555248	355950.810811	45.636033
3504.045491	355948.926530	45.641037
3504.013279	355967.203435	45.646042
3504.347237	355938.037986	45.651047
3504.033526	355941.014154	45.656052
3504.119203	355923.110585	45.661057
3504.306909	355925.829351	45.666061
3503.871039	355931.751370	45.671066
3504.279812	355932.297544	45.676071
3504.156007	355926.744003	45.681076
3504.218674	355929.838810	45.686081
3504.284269	355913.999713	45.691085
3504.037895	355910.119678	45.696090
3504.028606	355918.875356	45.701095
3504.187733	355911.953782	45.706100
3504.177342	355907.883753	45.711105
3504.357440	355905.743121	45.716109
3504.063321	355910.548462	45.721114
3504.017297	355901.852496	45.726119
3503.961787	355890.511417	45.731124
3503.943386	355887.231546	45.736129
3504.062014	355874.234251	45.741133
3504.048116	355893.755249	45.746138
3504.152741	355887.478492	45.751143
3504.041897	355884.976680	45.756148
3504.198669	355882.254426	45.761153
3504.211864	355887.825531	45.766157
3504.278038	355888.756690	45.771162
3504.292912	355870.355331	45.776167
3504.100610	355862.700410	45.781172
3504.039434	355855.533724	45.786177
3504.256293	355844.963921	45.791181
3503.930726	355852.039130	45.796186
3504.066972	355853.315487	45.801191
3504.263209	355856.974493	45.806196
3503.919082	355848.681917	45.811201
3503.854448	355851.796853	45.816205
3503.964594	355854.171610	45.821210
3504.074971	355846.112564	45.826215
3503.613713	355835.039199	45.831220
3503.625010	355843.486258	45.836225
3503.950561	355849.745987	45.841229
3504.024864	355854.747575	45.846234
3503.824272	355836.965574	45.851239
3503.539344	355832.888041	45.856244
3503.761688	355855.603632	45.861249
3503.918617	355865.249179	45.866253
3503.975017	355867.123467	45.871258
3504.108186	355857.304894	45.876263
3503.643954	355840.022638	45.881268
3503.707025	355847.545375	45.886273
3503.673243	355850.553641	45.891277
3503.607467	355876.826621	45.896282
3504.054108	355881.133142	45.901287
3504.109504	355873.184584	45.906292
3504.338013	355856.937994	45.911297
3504.300209	355840.199084	45.916301
3503.954594	355849.287872	45.921306
3504.236188	355846.520435	45.926311
3504.041072	355841.868845	45.931316
3503.901889	355850.161553	45.936321
3503.940871	355843.131721	45.941325
3503.599712	355853.034146	45.946330
3503.868716	355854.213173	45.951335
3504.130147	355850.481892	45.956340
3504.159168	355866.738744	45.961345
3504.412164	355841.123339	45.966349
3503.831341	355832.842730	45.971354
3504.005186	355819.378624	45.976359
3504.209206	355834.564446	45.981364
3503.842127	355835.207820	45.986369
3504.572571	355821.070418	45.991373
3504.530939	355823.367376	45.996378
3504.434789	355818.140278	46.001383
3504.187858	355810.061365	46.006388
3504.287451	355788.720038	46.011393
3504.295363	355782.127729	46.016397
3504.062144	355790.460760	46.021402
3504.237765	355793.843099	46.026407
3504.142249	355761.182687	46.031412
3504.400011	355756.077774	46.036417
3504.366693	355753.970872	46.041421
3503.983917	355760.749758	46.046426
3504.181530	355757.283042	46.051431
3504.097160	355765.719788	46.056436
3504.147409	355750.442928	46.061441
3504.285780	355739.045718	46.066445
3503.561590	355734.961272	46.071450
3503.865997	355724.097673	46.076455
3503.770459	355724.876261	46.081460
3504.012610	355722.624019	46.086465
3503.918696	355719.050695	46.091469
3504.167624	355724.177380	46.096474
3504.302707	355717.132339	46.101479
3503.983623	355722.577852	46.106484
3503.920714	355721.188178	46.111489
3504.091205	355717.216781	46.116493
3503.833596	355735.402159	46.121498
3504.068898	355732.183965	46.126503
3504.093625	355732.256438	46.131508
3504.254015	355720.270433	46.136513
3503.946320	355716.654559	46.141517
3503.678338	355719.674407	46.146522
3503.977227	355699.523054	46.151527
3503.704509	355709.720067	46.156532
3503.717210	355709.107337	46.161537
3503.742603	355714.472947	46.166541
3503.729280	355713.584400	46.171546
3504.109009	355698.891647	46.176551
3504.020667	355703.893513	46.181556
3503.942386	355720.752685	46.186561
3504.156694	355710.895808	46.191565
3503.905590	355718.595472	46.196570
3504.184348	355719.493028	46.201575
3503.878544	355716.792993	46.206580
3503.670471	355724.842129	46.211585
3503.989761	355712.856451	46.216589
3503.472580	355727.901830	46.221594
3503.848065	355724.050717	46.226599
3503.888387	355723.815345	46.231604
3503.961009	355728.842660	46.236609
3504.017795	355719.417859	46.241613
3504.067932	355727.629762	46.246618
3503.956316	355718.104341	46.251623
3504.007194	355727.715782	46.256628
3503.873834	355733.488210	46.261633
3504.399292	355720.477460	46.266637
3504.013607	355713.387501	46.271642
3504.040071	355688.138656	46.276647
3503.907545	355688.235988	46.281652
3503.895272	355687.016447	46.286657
3504.047626	355690.987781	46.291661
3503.794232	355689.551874	46.296666
3503.819375	355687.104900	46.301671
3503.788029	355688.942169	46.306676
3504.059642	355706.967552	46.311681
3504.106811	355700.139992	46.316685
3503.743004	355696.456642	46.321690
3504.026839	355689.031807	46.326695
3504.071492	355696.099409	46.331700
3504.162246	355699.495170	46.336705
3504.085982	355699.430917	46.341709
3503.973396	355709.653513	46.346714
3504.040496	355676.407478	46.351719
3503.735653	355679.814880	46.356724
3503.769637	355676.577611	46.361729
3503.942474	355667.159904	46.366733
3503.969219	355677.411377	46.371738
3504.143429	355672.217870	46.376743
3504.074812	355668.131578	46.381748
3504.096668	355675.075545	46.386753
3504.361647	355676.051626	46.391757
3504.084385	355675.484734	46.396762
3503.984733	355676.823835	46.401767
3504.132493	355678.301963	46.406772
3503.936812	355668.204511	46.411777
3504.133358	355648.705524	46.416781
3504.011984	355648.292126	46.421786
3504.234482	355646.195677	46.426791
3504.131935	355647.509789	46.431796
3503.828088	355640.585021	46.436801
3504.094494	355639.397769	46.441805
3504.012758	355655.188680	46.446810
3503.842313	355638.368879	46.451815
3503.720008	355651.341441	46.456820
3503.427090	355661.261726	46.461825
3504.063062	355644.670723	46.466829
3504.116094	355661.101984	46.471834
3503.952802	355655.503759	46.476839
3503.967402	355665.248188	46.481844
3503.858276	355651.319805	46.486849
3504.003249	355662.061557	46.491853
3503.663908	355657.865371	46.496858
3503.836790	355646.488133	46.501863
3503.875353	355659.002641	46.506868
3503.740134	355650.575216	46.511873
3504.321368	355651.374061	46.516877
3503.981725	355660.869111	46.521882
3504.085582	355646.932506	46.526887
3503.854398	355638.316662	46.531892
3503.842633	355635.697382	46.536897
3503.997584	355631.321262	46.541901
3503.823012	355633.359312	46.546906
3503.957241	355626.976050	46.551911
3504.006317	355629.233229	46.556916
3503.704457	355640.096520	46.561921
3503.994305	355634.273969	46.566925
3503.687988	355639.284851	46.571930
3503.957513	355628.961160	46.576935
3504.112087	355637.131120	46.581940
3504.274570	355647.183004	46.586945
3504.347831	355643.048833	46.591949
3504.022117	355649.716920	46.596954
3504.096883	355636.370222	46.601959
3504.130404	355613.665056	46.606964
3503.870713	355605.384542	46.611969
3503.931689	355607.258116	46.616973
3503.748289	355610.697221	46.621978
3503.857506	355601.874870	46.626983
3504.105174	355608.910391	46.631988
3503.843599	355609.155365	46.636993
3503.978163	355607.938058	46.641997
3503.911832	355613.623558	46.647002
3504.276724	355608.807075	46.652007
3504.514464	355617.650996	46.657012
3504.038878	355622.612293	46.662017
3504.272608	355609.800321	46.667021
3504.156208	355596.178452	46.672026
3504.426017	355580.383314	46.677031
3504.385680	355585.759328	46.682036
3504.352974	355578.944379	46.687041
3504.518085	355573.039747	46.692045
3503.979499	355564.421588	46.697050
3503.905876	355538.297799	46.702055
3504.010999	355545.763037	46.707060
3504.081519	355548.932971	46.712065
3504.036303	355544.054070	46.717069
3503.992234	355547.522051	46.722074
3504.281597	355544.956957	46.727079
3504.066983	355547.790240	46.732084
3504.126970	355545.490442	46.737089
3504.119206	355525.463841	46.742093
3503.953957	355524.090340	46.747098
3504.356599	355515.018002	46.752103
3504.020130	355527.897209	46.757108
3503.970578	355513.832128	46.762113
3503.911209	355515.902869	46.767117
3503.861762	355530.670778	46.772122
3504.325271	355519.502053	46.777127
3504.089067	355523.534824	46.782132
3504.045830	355527.002674	46.787137
3504.326329	355512.656383	46.792141
3503.708852	355503.821650	46.797146
3504.082919	355484.472676	46.802151
3504.242166	355493.125440	46.807156
3504.127687	355481.004691	46.812161
3504.217942	355487.047178	46.817165
3503.707267	355485.931869	46.822170
3503.916336	355478.340683	46.827175
3503.775758	355486.226496	46.832180
3503.941696	355499.866085	46.837185
3504.139159	355490.953420	46.842189
3504.071888	355500.583581	46.847194
3503.798119	355500.397860	46.852199
3504.060995	355496.997155	46.857204
3504.123008	355487.215207	46.862209
3503.922959	355470.501824	46.867213
3503.742047	355475.212965	46.872218
3504.104271	355454.898813	46.877223
3503.735114	355458.061912	46.882228
3504.026490	355458.117681	46.887233
3504.279645	355460.622540	46.892237
3503.981900	355475.964133	46.897242
3503.750544	355465.719590	46.902247
3504.020635	355455.166739	46.907252
3503.615479	355467.496955	46.912257
3504.006779	355470.565287	46.917261
3503.857845	355473.464537	46.922266
3503.990303	355462.831652	46.927271
3503.959804	355478.512724	46.932276
3503.884160	355480.662384	46.937281
3503.948311	355469.531330	46.942285
3504.042468	355471.552354	46.947290
3504.214015	355469.133123	46.952295
3503.979981	355479.960277	46.957300
3504.320161	355467.207787	46.962305
3504.267189	355435.634723	46.967309
3503.897907	355450.962184	46.972314
3504.140464	355436.749111	46.977319
3504.127194	355440.822992	46.982324
3504.052561	355440.809379	46.987329
3504.338860	355438.473800	46.992333
3504.240060	355436.631721	46.997338
3503.948019	355414.970420	47.002343
3503.840573	355409.210649	47.007348
3503.712035	355418.392439	47.012353
3503.748894	355407.647413	47.017357
3503.671163	355413.589221	47.022362
3504.237632	355420.370785	47.027367
3504.204069	355414.853819	47.032372
3503.744948	355427.014436	47.037377
3504.208920	355418.924874	47.042381
3504.383623	355409.201443	47.047386
3504.187643	355415.314635	47.052391
3504.215898	355420.756168	47.057396
3504.577097	355407.669512	47.062401
3504.209845	355395.970428	47.067405
3504.237799	355393.675686	47.072410
3504.253153	355378.327886	47.077415
3504.358827	355377.395073	47.082420
3503.851705	355382.870347	47.087425
3504.061101	355373.523151	47.092429
3504.077612	355359.574827	47.097434
3504.207502	355347.160931	47.102439
3504.030414	355341.666646	47.107444
3503.760660	355346.111910	47.112449
3504.225608	355349.779371	47.117453
3503.852833	355354.011884	47.122458
3504.041199	355346.907472	47.127463
3504.216002	355355.939527	47.132468
3504.026952	355363.527640	47.137473
3504.087328	355357.486849	47.142477
3504.246326	355352.651993	47.147482
3504.145512	355339.994633	47.152487
3503.930600	355323.741624	47.157492
3503.748131	355321.989112	47.162497
3504.133452	355315.209840	47.167501
3503.618512	355314.884103	47.172506
3504.039090	355311.407558	47.177511
3503.837706	355316.885405	47.182516
3503.783453	355323.179791	47.187521
3503.771196	355321.934790	47.192525
3503.639202	355325.009510	47.197530
3503.832109	355317.955273	47.202535
3503.522182	355320.243769	47.207540
3503.665023	355317.829069	47.212545
3503.981432	355319.662275	47.217549
3503.757660	355328.808239	47.222554
3503.973093	355325.440470	47.227559
3504.087342	355331.682770	47.232564
3503.985096	355330.019371	47.237569
3504.094118	355336.618775	47.242573
3504.064537	355327.589282	47.247578
3504.382404	355327.844452	47.252583
3504.277860	355329.031644	47.257588
3503.926505	355335.474790	47.262593
3504.067745	355322.880955	47.267597
3504.366785	355310.694796	47.272602
3504.139693	355310.374453	47.277607
3504.049169	355302.296183	47.282612
3504.200051	355304.715423	47.287617
3504.315735	355305.002554	47.292621
3503.954418	355307.630005	47.297626
3504.117231	355291.342722	47.302631
3504.037441	355299.142609	47.307636
3503.937643	355283.685741	47.312641
3504.149711	355270.291794	47.317645
3504.013141	355267.692224	47.322650
3504.259785	355268.085896	47.327655
3504.100275	355272.513739	47.332660
3503.854381	355266.648595	47.337665
3503.910241	355275.012357	47.342669
3504.341128	355270.414447	47.347674
3504.123388	355264.748440	47.352679
3504.006674	355264.207060	47.357684
3503.599155	355254.906468	47.362689
3503.949866	355247.623688	47.367693
3503.968143	355254.950006	47.372698
3503.968065	355245.966731	47.377703
3503.713286	355245.370831	47.382708
3503.847066	355241.557892	47.387713
3503.893151	355226.917746	47.392717
3503.927860	355238.338681	47.397722
3504.088256	355233.274556	47.402727
3504.232033	355238.265222	47.407732
3503.943134	355233.272122	47.412737
3504.065070	355231.649626	47.417741
3503.638601	355246.019145	47.422746
3503.952108	355243.424771	47.427751
3503.954878	355239.581645	47.432756
3503.884805	355239.592759	47.437761
3503.689928	355242.143005	47.442765
3503.888046	355253.665347	47.447770
3504.002475	355238.836261	47.452775
3504.220169	355244.018830	47.457780
3503.741201	355257.887674	47.462785
3504.320575	355244.486553	47.467789
3503.798881	355249.353380	47.472794
3503.931816	355234.215985	47.477799
3504.037907	355227.608085	47.482804
3503.950993	355222.252223	47.487809
3504.113781	355207.262792	47.492813
3503.744103	355208.695489	47.497818
3503.943635	355206.729895	47.502823
3503.831333	355214.000516	47.507828
3503.843644	355214.609371	47.512833
3504.307695	355204.509330	47.517837
3503.765863	355228.542083	47.522842
3503.749773	355212.308505	47.527847
3503.825669	355209.853485	47.532852
3503.947120	355216.527286	47.537857
3504.168687	355219.622466	47.542861
3503.828640	355224.689617	47.547866
3503.967948	355215.022641	47.552871
3503.998363	355220.972825	47.557876
3504.098685	355224.367105	47.562881
3504.495954	355217.764070	47.567885
3503.895495	355207.094301	47.572890
3504.049956	355198.417419	47.577895
3504.013847	355192.977178	47.582900
3504.286149	355193.570382	47.587905
3504.074385	355198.388219	47.592909
3503.882444	355194.601318	47.597914
3504.203378	355196.510159	47.602919
3504.082710	355203.222236	47.607924
3504.247651	355203.247095	47.612929
3504.421167	355189.019419	47.617933
3504.218862	355173.833208	47.622938
3504.166999	355159.488461	47.627943
3504.311782	355157.913248	47.632948
3503.989043	355143.687663	47.637953
3504.374530	355150.523321	47.642957
3503.976855	355158.449827	47.647962
3503.990912	355145.697914	47.652967
3504.231052	355129.474702	47.657972
3503.640355	355125.445449	47.662977
3503.917172	355122.347897	47.667981
3503.644931	355125.521145	47.672986
3504.123996	355117.251010	47.677991
3504.111668	355133.132904	47.682996
3503.874116	355120.929731	47.688001
3504.047809	355126.602790	47.693005
3504.048196	355133.931954	47.698010
3504.001983	355134.346473	47.703015
3504.070282	355130.798362	47.708020
3503.718866	355131.032092	47.713025
3503.948576	355124.939056	47.718029
3503.764921	355140.110023	47.723034
3504.228899	355128.228578	47.728039
3504.223925	355125.404610	47.733044
3503.964444	355118.065580	47.738049
3504.072654	355102.575775	47.743053
3503.671470	355107.627154	47.748058
3503.782905	355097.964562	47.753063
3503.664105	355101.215349	47.758068
3503.677724	355097.319599	47.763073
3503.957753	355124.021825	47.768077
3503.874328	355111.488902	47.773082
3503.758046	355105.883185	47.778087
3503.696566	355115.563401	47.783092
3503.822720	355142.213596	47.788097
3504.177527	355131.876324	47.793101
3503.996275	355116.305039	47.798106
3503.882243	355107.288857	47.803111
3504.025211	355108.462376	47.808116
3503.783966	355104.377879	47.813121
3504.209452	355101.027788	47.818125
3503.939651	355113.107654	47.823130
3503.810048	355108.776471	47.828135
3503.934202	355117.027669	47.833140
3503.953440	355122.267071	47.838145
3503.868311	355113.577153	47.843149
3503.887450	355124.008080	47.848154
3503.916502	355124.461599	47.853159
3503.876677	355117.087845	47.858164
3503.813858	355119.973501	47.863169
3503.742374	355113.928077	47.868173
3503.625440	355125.067626	47.873178
3503.845368	355121.190162	47.878183
3504.237560	355125.429009	47.883188
3503.984863	355132.391004	47.888193
3504.267740	355126.416806	47.893197
3503.792712	355133.057667	47.898202
3503.842823	355129.334291	47.903207
3504.022798	355136.202439	47.908212
3503.898973	355131.310477	47.913217
3504.113669	355115.193077	47.918221
3503.694705	355110.627703	47.923226
3503.799398	355114.962897	47.928231
3503.729564	355105.787036	47.933236
3503.814961	355111.626746	47.938241
3503.893935	355093.164077	47.943245
3504.131090	355112.976518	47.948250
3503.966275	355103.383046	47.953255
3504.494173	355109.992609	47.958260
3504.132253	355105.341871	47.963265
3503.954528	355103.334116	47.968269
3503.887486	355116.399872	47.973274
3503.966983	355112.900887	47.978279
3504.419714	355103.566073	47.983284
3504.141116	355111.957285	47.988289
3504.354261	355085.584342	47.993293
3503.954058	355066.459403	47.998298
3503.909817	355079.012592	48.003303
3503.756324	355081.887136	48.008308
3503.769818	355071.247526	48.013313
3503.943268	355070.354891	48.018317
3503.672351	355074.673120	48.023322
3503.576728	355083.773421	48.028327
3503.859712	355084.568527	48.033332
3503.859444	355082.176438	48.038337
3504.435173	355074.298193	48.043341
3504.401050	355086.646192	48.048346
3504.241189	355075.219633	48.053351
3504.372862	355086.574376	48.058356
3504.029255	355080.648312	48.063361
3504.406440	355052.162636	48.068365
3503.858495	355050.162507	48.073370
3503.895640	355038.984731	48.078375
3504.312571	355046.706134	48.083380
3504.051649	355049.114139	48.088385
3504.230756	355048.475096	48.093389
3504.029054	355059.475367	48.098394
3503.812960	355048.795701	48.103399
3504.136102	355043.578587	48.108404
3504.039516	355030.818688	48.113409
3504.147689	355018.535389	48.118413
3504.036145	355018.985686	48.123418
3503.894133	355013.918447	48.128423
3504.256417	355016.202487	48.133428
3504.119140	355009.633030	48.138433
3504.357661	354999.644947	48.143437
3504.066969	355007.452769	48.148442
3504.004094	354997.817714	48.153447
3503.840847	354987.740448	48.158452
3503.839847	354974.481900	48.163457
3503.654580	354973.187894	48.168461
3503.648164	354990.824855	48.173466
3503.937685	354997.472115	48.178471
3504.061296	355002.135160	48.183476
3503.730769	354993.407668	48.188481
3503.726278	354990.481822	48.193485
3503.814221	354996.244797	48.198490
3503.734862	354998.980383	48.203495
3503.918547	355003.379445	48.208500
3503.663975	355006.880738	48.213505
3504.080183	355004.982679	48.218509
3503.728361	354998.268996	48.223514
3504.221999	354998.801765	48.228519
3504.072492	354978.619217	48.233524
3503.804784	354980.595670	48.238529
3503.911770	354982.716481	48.243533
3503.853682	354992.930605	48.248538
3504.003078	354982.473082	48.253543
3504.146748	354991.408329	48.258548
3504.027606	354990.765536	48.263553
3503.920133	354989.459233	48.268557
3503.533850	354993.363078	48.273562
3504.091701	354994.292875	48.278567
3503.984782	354992.146679	48.283572
3503.445301	354996.863650	48.288577
3503.815447	354989.755901	48.293581
3504.335801	354986.365356	48.298586
3504.092891	354992.994990	48.303591
3504.015972	354991.403922	48.308596
3503.859880	355000.106619	48.313601
3503.857878	354990.258351	48.318605
3503.921471	355010.225512	48.323610
3503.955324	354995.841720	48.328615
3504.357704	354975.190198	48.333620
3503.800809	354972.886096	48.338625
3504.028026	354971.832269	48.343629
3503.961165	354966.345967	48.348634
3504.002073	354962.700380	48.353639
3504.217654	354970.453624	48.358644
3503.867088	354973.181187	48.363649
3504.168620	354953.436301	48.368653
3503.971165	354969.347511	48.373658
3504.012854	354963.258730	48.378663
3504.338264	354965.319564	48.383668
3504.100816	354958.002476	48.388673
3504.197215	354936.457708	48.393677
3503.860111	354936.434689	48.398682
3504.138483	354932.242588	48.403687
3504.013993	354935.290695	48.408692
3503.987102	354935.422226	48.413697
3504.193087	354928.722150	48.418701
3503.872320	354945.543564	48.423706
3504.088055	354941.717647	48.428711
3504.102968	354935.862134	48.433716
3503.950638	354936.344327	48.438721
3503.936938	354920.899187	48.443725
3504.209048	354912.330903	48.448730
3503.933353	354898.046915	48.453735
3503.703665	354908.593566	48.458740
3503.838637	354900.454137	48.463745
3504.207768	354898.665311	48.468749
3503.894203	354902.684911	48.473754
3503.819799	354906.106833	48.478759
3504.093145	354910.160897	48.483764
3503.916685	354908.127486	48.488769
3503.724322	354902.457427	48.493773
3503.802205	354907.076812	48.498778
3503.959454	354913.083327	48.503783
3504.071224	354911.106147	48.508788
3503.860676	354907.780242	48.513793
3504.242389	354905.836735	48.518797
3504.052471	354908.437111	48.523802
3504.127897	354906.694714	48.528807
3504.279012	354884.810442	48.533812
3503.819286	354887.173535	48.538817
3504.114169	354874.351713	48.543821
3504.096851	354876.364934	48.548826
3504.136255	354863.023624	48.553831
3503.929172	354875.246324	48.558836
3503.708752	354880.574533	48.563841
3504.203671	354870.342303	48.568845
3503.972021	354880.711130	48.573850
3504.080389	354882.628136	48.578855
3504.201555	354879.020753	48.583860
3504.256119	354871.072172	48.588865
3504.376542	354850.312479	48.593869
3503.731719	354850.770733	48.598874
3503.912884	354840.079121	48.603879
3504.248759	354847.711573	48.608884
3503.967955	354844.320424	48.613889
3504.072576	354830.485270	48.618893
3504.137399	354845.438904	48.623898
3503.725933	354842.119307	48.628903
3503.982790	354848.466366	48.633908
3503.869673	354855.711717	48.638913
3504.101323	354845.419305	48.643917
3503.882460	354854.691821	48.648922
3504.131149	354833.708256	48.653927
3504.049433	354827.409929	48.658932
3503.661132	354818.615194	48.663937
3503.863470	354814.918628	48.668941
3503.944174	354815.262189	48.673946
3503.768649	354815.595358	48.678951
3503.983269	354819.760507	48.683956
3503.957857	354820.171741	48.688961
3504.374428	354813.311116	48.693965
3503.807594	354814.724093	48.698970
3503.853586	354809.678011	48.703975
3504.078721	354814.299575	48.708980
3503.813949	354823.172175	48.713985
3504.103980	354814.550143	48.718989
3503.834909	354813.549318	48.723994
3503.781451	354823.050179	48.728999
3503.978711	354814.442813	48.734004
3503.839123	354826.502162	48.739009
3504.004544	354829.580793	48.744013
3503.519646	354836.681328	48.749018
3503.839956	354834.493038	48.754023
3504.019438	354829.502202	48.759028
3503.935610	354836.488439	48.764033
3504.330526	354833.448548	48.769037
3503.943521	354803.149435	48.774042
3503.751215	354799.286216	48.779047
3504.052179	354787.964886	48.784052
3503.792155	354795.946034	48.789057
3504.188249	354787.968899	48.794061
3503.899435	354804.276333	48.799066
3504.153440	354803.599998	48.804071
3503.947231	354795.590833	48.809076
3503.847188	354806.346050	48.814081
3504.373516	354808.400578	48.819085
3504.061487	354800.637180	48.824090
3503.973991	354798.055278	48.829095
3504.185264	354805.402048	48.834100
3503.750481	354794.553310	48.839105
3504.049291	354776.412057	48.844109
3504.020935	354773.719009	48.849114
3503.993909	354763.340229	48.854119
3503.905714	354758.035418	48.859124
3503.815341	354768.636422	48.864129
3504.052344	354767.250209	48.869133
3503.963601	354777.901851	48.874138
3503.851886	354771.048387	48.879143
3503.875734	354778.755623	48.884148
3503.844456	354780.491119	48.889153
3504.438473	354766.960315	48.894157
3503.764605	354776.762850	48.899162
3504.065454	354773.177953	48.904167
3504.019354	354771.531109	48.909172
3503.923506	354774.040275	48.914177
3503.891423	354779.516863	48.919181
3504.041930	354780.612853	48.924186
3503.875187	354773.310010	48.929191
3503.767318	354758.108747	48.934196
3503.532960	354773.211491	48.939201
3503.735762	354764.399651	48.944205
3503.819452	354779.757500	48.949210
3503.985886	354783.192256	48.954215
3504.022891	354789.243243	48.959220
3503.866017	354787.155834	48.964225
3503.995017	354776.090724	48.969229
3503.930498	354763.274791	48.974234
3503.923114	354746.454368	48.979239
3503.899662	354752.718507	48.984244
3503.942116	354757.445301	48.989249
3504.303964	354744.002090	48.994253
3504.069314	354755.134879	48.999258
3503.754194	354757.729606	49.004263
3504.032954	354747.277035	49.009268
3503.963243	354750.520084	49.014273
3504.141134	354747.310905	49.019277
3504.239775	354761.444856	49.024282
3504.218475	354748.062215	49.029287
3504.148240	354723.108117	49.034292
3503.837805	354716.082469	49.039297
3504.076239	354701.182727	49.044301
3504.070460	354712.813770	49.049306
3503.835117	354714.912361	49.054311
3503.802944	354716.113576	49.059316
3503.633043	354721.790099	49.064321
3504.089462	354713.167196	49.069325
3504.014582	354712.899134	49.074330
3503.806251	354725.122066	49.079335
3503.774226	354721.055362	49.084340
3503.746260	354722.815785	49.089345
3504.034111	354708.671697	49.094349
3504.153928	354724.125648	49.099354
3503.949798	354724.310646	49.104359
3503.869861	354731.703463	49.109364
3504.109900	354726.346761	49.114369
3504.096852	354710.545173	49.119373
3503.969049	354727.437949	49.124378
3504.210899	354711.774208	49.129383
3504.319853	354697.047626	49.134388
3504.026311	354692.157002	49.139393
3504.231597	354682.733984	49.144397
3503.800144	354685.118066	49.149402
3504.032566	354681.849365	49.154407
3504.005390	354684.933001	49.159412
3503.840059	354686.206165	49.164417
3504.119118	354697.359553	49.169421
3503.766024	354702.657857	49.174426
3503.955119	354693.186503	49.179431
3504.059467	354688.589263	49.184436
3503.765595	354696.804815	49.189441
3504.168909	354691.753134	49.194445
3504.251291	354684.512692	49.199450
3503.959849	354676.440636	49.204455
3504.031364	354666.758825	49.209460
3503.925604	354671.050978	49.214465
3504.260852	354667.028006	49.219469
3503.908399	354668.203507	49.224474
3504.108092	354669.775250	49.229479
3504.325734	354664.320288	49.234484
3504.184386	354670.221341	49.239489
3504.124581	354654.045395	49.244493
3504.063578	354637.793286	49.249498
3503.824577	354625.895610	49.254503
3504.094968	354628.754068	49.259508
3503.861882	354621.130857	49.264513
3504.144003	354629.535304	49.269517
3503.992661	354631.671517	49.274522
3504.280513	354636.435876	49.279527
3504.087273	354632.725484	49.284532
3504.103558	354631.094223	49.289537
3504.413827	354622.061779	49.294541
3504.147130	354600.447025	49.299546
3504.145833	354600.243676	49.304551
3503.989241	354587.645845	49.309556
3503.987222	354596.731435	49.314561
3504.118578	354583.986289	49.319565
3503.879511	354593.618330	49.324570
3504.192562	354597.386204	49.329575
3503.800948	354594.241595	49.334580
3504.177276	354601.714996	49.339585
3504.497544	354587.616648	49.344589
3504.049339	354564.961720	49.349594
3504.143714	354558.457381	49.354599
3504.335782	354552.675615	49.359604
3504.193314	354551.451179	49.364609
3504.295121	354559.527858	49.369613
3504.358022	354554.071897	49.374618
3504.304365	354528.580657	49.379623
3504.019677	354523.510476	49.384628
3503.861770	354521.728605	49.389633
3504.335437	354527.939634	49.394637
3504.065899	354513.781810	49.399642
3504.483739	354525.167787	49.404647
3504.117098	354525.149436	49.409652
3503.891083	354512.486215	49.414657
3503.860521	354479.102148	49.419661
3503.784077	354486.876181	49.424666
3503.706544	354484.954359	49.429671
3503.908111	354484.947980	49.434676
3503.858032	354475.463498	49.439681
3503.942681	354472.981610	49.444685
3503.897074	354485.713302	49.449690
3503.801667	354486.924519	49.454695
3504.169384	354490.429271	49.459700
3503.905572	354494.695526	49.464705
3504.167399	354477.756112	49.469709
3504.062384	354485.331070	49.474714
3503.918720	354489.069355	49.479719
3504.317995	354491.398469	49.484724
3503.942859	354492.908394	49.489729
3504.100412	354482.067748	49.494733
3504.189715	354485.769205	49.499738
3503.936524	354462.599876	49.504743
3503.779235	354460.512519	49.509748
3503.960362	354450.507953	49.514753
3504.161223	354451.570540	49.519757
3504.297135	354450.200300	49.524762
3504.280613	354457.939415	49.529767
3504.249928	354460.667335	49.534772
3504.139464	354461.371955	49.539777
3504.091239	354453.490455	49.544781
3503.638682	354432.388541	49.549786
3503.768879	354440.308057	49.554791
3503.769826	354451.200076	49.559796
3503.671423	354452.539012	49.564801
3503.719059	354458.868295	49.569805
3503.525535	354466.304554	49.574810
3503.861275	354465.946130	49.579815
3503.844301	354466.177890	49.584820
3504.048159	354461.437655	49.589825
3503.846089	354462.284000	49.594829
3504.065762	354470.138469	49.599834
3503.951889	354467.815209	49.604839
3504.070032	354452.399984	49.609844
3503.865236	354436.577726	49.614849
3504.013030	354432.329879	49.619853
3503.869548	354438.943866	49.624858
3503.677008	354437.956384	49.629863
3503.940826	354432.494098	49.634868
3503.589609	354441.253183	49.639873
3503.724602	354434.971448	49.644877
3503.605456	354443.159420	49.649882
3503.659433	354460.048997	49.654887
3504.172798	354469.765706	49.659892
3503.892885	354465.025600	49.664897
3504.169422	354445.335368	49.669901
3503.902016	354444.334271	49.674906
3503.811844	354433.201940	49.679911
3504.122090	354433.025688	49.684916
3503.673195	354446.711854	49.689921
3503.789878	354436.030352	49.694925
3503.625645	354440.051830	49.699930
3504.003705	354439.228635	49.704935
3504.007158	354440.653265	49.709940
3503.501087	354448.953300	49.714945
3504.010625	354431.694774	49.719949
3503.922544	354437.561985	49.724954
3503.629427	354450.307363	49.729959
3503.920923	354449.548751	49.734964
3503.793449	354450.815935	49.739969
3504.049231	354439.883405	49.744973
3503.894896	354447.186228	49.749978
3503.759232	354438.173348	49.754983
3504.008890	354443.452740	49.759988
3503.470156	354451.452551	49.764993
3503.935679	354450.462837	49.769997
3504.111229	354448.908188	49.775002
3503.734135	354449.604059	49.780007
3504.144013	354445.951006	49.785012
3503.776551	354457.893770	49.790017
3503.959604	354451.273604	49.795021
3504.057971	354463.931644	49.800026
3503.973269	354461.527425	49.805031
3504.022855	354456.709781	49.810036
3503.509756	354460.531918	49.815041
3503.971756	354456.056261	49.820045
3504.022028	354455.870209	49.825050
3504.045795	354449.835098	49.830055
3504.247836	354456.674400	49.835060
3503.950865	354430.509007	49.840065
3503.961632	354427.784307	49.845069
3503.765134	354429.011506	49.850074
3503.970189	354411.113985	49.855079
3504.079060	354420.462015	49.860084
3503.882065	354429.374866	49.865089
3504.294857	354420.046242	49.870093
3504.230426	354427.894731	49.875098
3503.985246	354427.882628	49.880103
3504.439205	354434.962048	49.885108
3503.838100	354418.973393	49.890113
3504.226286	354405.958562	49.895117
3503.874540	354397.870546	49.900122
3504.038418	354389.421080	49.905127
3504.206893	354380.309213	49.910132
3504.092123	354383.126776	49.915137
3504.003219	354379.527118	49.920141
3504.550850	354370.100822	49.925146
3504.070871	354372.899772	49.930151
3504.176518	354381.459401	49.935156
3504.027187	354357.230200	49.940161
3503.984883	354349.831279	49.945165
3504.062035	354356.817581	49.950170
3503.845369	354352.678241	49.955175
3504.186136	354354.787570	49.960180
3503.970870	354363.652422	49.965185
3503.958856	354358.259181	49.970189
3503.818632	354357.416120	49.975194
3503.919124	354357.400271	49.980199
3503.756866	354348.976906	49.985204
3503.665314	354353.801267	49.990209
3504.008585	354354.637753	49.995213
3503.884511	354346.971819	50.000218
3503.848917	354347.053830	50.005223
3504.260325	354346.123566	50.010228
3503.988612	354355.429975	50.015233
3504.081543	354351.114448	50.020237
3503.828958	354361.690280	50.025242
3503.596149	354349.867908	50.030247
3503.688419	354355.375782	50.035252
3503.718016	354361.936969	50.040257
3504.223405	354361.678971	50.045261
3503.738725	354365.929254	50.050266
3504.176366	354361.177501	50.055271
3504.274136	354341.337347	50.060276
3503.842684	354335.526879	50.065281
3503.820663	354325.757994	50.070285
3503.883428	354326.180742	50.075290
3504.020542	354326.769879	50.080295
3503.908956	354315.310070	50.085300
3503.730876	354327.706457	50.090305
3503.904181	354323.250977	50.095309
3504.151542	354320.667014	50.100314
3504.027289	354328.397730	50.105319
3504.537196	354324.448917	50.110324
3503.953605	354328.562146	50.115329
3503.821108	354326.725353	50.120333
3503.765982	354326.148778	50.125338
3503.694595	354318.067328	50.130343
3504.039482	354324.018802	50.135348
3503.960460	354336.959404	50.140353
3503.952056	354323.574614	50.145357
3503.880150	354321.321060	50.150362
3503.884101	354298.670885	50.155367
3503.997074	354309.367082	50.160372
3503.918369	354297.876623	50.165377
3504.188017	354294.296625	50.170381
3504.203180	354301.928959	50.175386
3503.583321	354304.902719	50.180391
3504.078061	354293.677893	50.185396
3504.083635	354301.973417	50.190401
3503.749352	354300.830195	50.195405
3503.915874	354306.020949	50.200410
3503.875477	354305.187555	50.205415
3504.102879	354308.892644	50.210420
3504.195148	354309.361625	50.215425
3503.995273	354315.704604	50.220429
3503.962147	354309.525777	50.225434
3504.146938	354296.492174	50.230439
3504.041284	354272.892253	50.235444
3503.871236	354278.161663	50.240449
3503.821224	354268.575336	50.245453
3503.921105	354254.359042	50.250458
3503.872918	354267.218441	50.255463
3504.101833	354260.438306	50.260468
3503.958784	354275.221374	50.265473
3504.181243	354265.617422	50.270477
3504.264061	354274.104331	50.275482
3503.788968	354272.652532	50.280487
3504.000223	354269.310804	50.285492
3504.011150	354278.318057	50.290497
3503.974057	354281.301489	50.295501
3503.710394	354277.780348	50.300506
3503.860323	354275.339030	50.305511
3503.755585	354270.520315	50.310516
3503.909013	354275.382304	50.315521
3503.699287	354265.770326	50.320525
3503.796896	354274.534836	50.325530
3503.816859	354267.329652	50.330535
3504.170019	354270.200495	50.335540
3503.729307	354276.530652	50.340545
3504.174108	354252.105684	50.345549
3504.196454	354244.442038	50.350554
3503.946428	354242.318434	50.355559
3503.852013	354244.547460	50.360564
3503.770762	354243.847769	50.365569
3504.431286	354231.018884	50.370573
3503.952711	354243.666386	50.375578
3503.924709	354242.958277	50.380583
3504.269862	354240.944178	50.385588
3503.857989	354247.066188	50.390593
3503.805185	354242.341057	50.395597
3504.147881	354244.679126	50.400602
3503.965459	354251.681028	50.405607
3503.801392	354239.695070	50.410612
3504.091584	354247.843813	50.415617
3504.030630	354226.476317	50.420621
3503.705851	354211.563672	50.425626
3504.056844	354209.523200	50.430631
3504.133100	354194.547153	50.435636
3503.949234	354206.257360	50.440641
3503.802254	354205.568059	50.445645
3503.941945	354200.990638	50.450650
3503.694776	354215.968325	50.455655
3503.897554	354210.973747	50.460660
3503.758812	354215.449295	50.465665
3503.836658	354204.366701	50.470669
3503.639034	354215.493753	50.475674
3503.716471	354222.047395	50.480679
3504.051769	354207.233995	50.485684
3503.893577	354216.598831	50.490689
3503.699842	354212.379507	50.495693
3504.190813	354210.647744	50.500698
3504.148771	354206.633481	50.505703
3504.223118	354209.675648	50.510708
3503.578412	354221.306007	50.515713
3503.672085	354215.234369	50.520717
3504.104209	354211.908621	50.525722
3503.965946	354208.723937	50.530727
3504.319209	354195.052900	50.535732
3503.847164	354177.007845	50.540737
3503.730251	354138.954586	50.545741
3503.643820	354109.549166	50.550746
3503.511350	354057.883051	50.555751
3503.509429	354008.206727	50.560756
3502.967496	353944.796834	50.565761
3503.039662	353864.798710	50.570765
3502.730081	353798.501598	50.575770
3502.468864	353712.499026	50.580775
3502.309097	353613.959213	50.585780
3501.909832	353522.837389	50.590785
3501.473909	353416.044365	50.595789
3501.488237	353300.781623	50.600794
3500.855683	353177.426140	50.605799
3500.420540	353055.591585	50.610804
3499.924406	352945.498675	50.615809
3499.752241	352813.442129	50.620813
3499.066285	352676.478319	50.625818
3498.383105	352548.548406	50.630823
3497.981676	352401.486220	50.635828
3497.392735	352270.690349	50.640833
3497.153793	352123.856205	50.645837
3497.070046	351975.062914	50.650842
3496.442079	351808.870966	50.655847
3495.895787	351660.735274	50.660852
3495.100727	351514.547273	50.665857
3494.710183	351332.104450	50.670861
3494.144034	351186.337474	50.675866
3493.349252	351013.908613	50.680871
3493.534143	350858.274454	50.685876
3492.552837	350686.764808	50.690881
3492.043751	350510.013454	50.695885
3491.069895	350351.812337	50.700890
3490.403207	350176.281005	50.705895
3490.172577	349994.826433	50.710900
3489.555066	349831.757227	50.715905
3489.207627	349643.906277	50.720909
3488.524279	349463.386857	50.725914
3487.776424	349283.564229	50.730919
3487.518244	349084.625914	50.735924
3486.668566	348916.042282	50.740929
3485.889733	348730.241642	50.745933
3485.315059	348551.458229	50.750938
3484.799343	348366.531041	50.755943
3484.186872	348172.557670	50.760948
3483.433269	347998.967509	50.765953
3482.963834	347795.603901	50.770957
3482.296089	347606.625917	50.775962
3481.468946	347427.904290	50.780967
3481.092794	347231.930501	50.785972
3480.007069	347044.874739	50.790977
3479.342465	346856.835498	50.795981
3479.026610	346651.432764	50.800986
3478.464607	346474.931508	50.805991
3477.959234	346283.836347	50.810996
3476.873910	346091.177806	50.816001
3476.407971	345880.043708	50.821005
3475.717794	345691.088392	50.826010
3475.062782	345503.679539	50.831015
3474.410004	345308.481065	50.836020
3473.195778	345121.515735	50.841025
3472.775379	344917.650571	50.846029
3472.191958	344750.336105	50.851034
3471.521306	344546.331042	50.856039
3471.060280	344359.295117	50.861044
3469.991577	344174.314601	50.866049
3469.526564	343985.140019	50.871053
3468.827553	343788.212964	50.876058
3468.393301	343607.253898	50.881063
3467.689283	343414.144484	50.886068
3467.071132	343217.584577	50.891073
3466.384220	343019.991280	50.896077
3465.877763	342829.368715	50.901082
3464.958145	342632.167298	50.906087
3464.523029	342426.081426	50.911092
3463.623725	342240.329997	50.916097
3462.944684	342040.925001	50.921101
3462.363905	341850.158392	50.926106
3461.388102	341648.660850	50.931111
3460.955967	341457.614976	50.936116
3460.008049	341259.879063	50.941121
3459.509192	341072.278955	50.946125
3458.887527	340881.744914	50.951130
3458.247111	340700.097084	50.956135
3457.854283	340501.176430	50.961140
3456.908708	340310.640949	50.966145
3456.346418	340121.520701	50.971149
3455.820925	339922.644647	50.976154
3454.897059	339726.961976	50.981159
3454.151913	339521.959163	50.986164
3453.743037	339335.408781	50.991169
3452.974700	339139.725170	50.996173
3452.433919	338938.837456	51.001178
3451.472796	338749.878011	51.006183
3450.778079	338549.140698	51.011188
3449.840668	338373.413498	51.016193
3449.599693	338174.410661	51.021197
3448.790689	337985.577670	51.026202
3448.010447	337799.794335	51.031207
3447.722456	337598.327918	51.036212
3447.094672	337406.460757	51.041217
3446.260931	337216.076619	51.046221
3445.593897	337015.024735	51.051226
3444.824276	336833.971914	51.056231
3444.703878	336616.718352	51.061236
3443.410169	336425.920993	51.066241
3442.530886	336235.286677	51.071245
3441.897981	336043.034536	51.076250
3441.304033	335867.984614	51.081255
3440.670763	335669.367217	51.086260
3440.050990	335482.431929	51.091265
3439.431281	335284.065831	51.096269
3438.858043	335103.486446	51.101274
3437.734504	334908.813851	51.106279
3437.270905	334712.050681	51.111284
3436.582985	334541.467258	51.116289
3435.891048	334341.073253	51.121293
3435.335212	334145.494100	51.126298
3434.333270	333965.055888	51.131303
3434.067290	333780.071194	51.136308
3433.422489	333593.949389	51.141313
3432.771466	333404.034846	51.146317
3431.802272	333207.398278	51.151322
3431.422117	333019.043723	51.156327
3431.037761	332832.649606	51.161332
3429.979349	332647.125322	51.166337
3429.451363	332447.820154	51.171341
3429.043921	332260.511695	51.176346
3428.144070	332074.757189	51.181351
3427.474757	331872.290472	51.186356
3426.612577	331683.015736	51.191361
3425.814923	331494.875939	51.196365
3425.184407	331292.223258	51.201370
3424.426621	331121.795413	51.206375
3423.638788	330920.057630	51.211380
3422.982978	330741.262297	51.216385
3422.098753	330556.468887	51.221389
3422.070609	330370.826804	51.226394
3420.937283	330195.007976	51.231399
3420.445392	330006.586899	51.236404
3419.860164	329820.395051	51.241409
3419.328048	329620.497282	51.246413
3418.423866	329442.680096	51.251418
3417.455773	329254.637940	51.256423
3417.175791	329070.789155	51.261428
3415.958452	328900.148847	51.266433
3415.624961	328714.245446	51.271437
3415.386717	328533.927642	51.276442
3414.439712	328339.795056	51.281447
3413.525502	328158.335733	51.286452
3413.057014	327981.744702	51.291457
3412.622345	327779.739010	51.296461
3411.771690	327602.774730	51.301466
3410.906466	327429.631346	51.306471
3410.795997	327229.558847	51.311476
3409.912313	327045.978930	51.316481
3409.376124	326851.701304	51.321485
3408.536265	326654.008631	51.326490
3407.751609	326464.632245	51.331495
3407.292330	326297.430818	51.336500
3406.418857	326115.425681	51.341505
3406.094125	325918.820917	51.346509
3405.152099	325733.006691	51.351514
3403.929695	325558.260791	51.356519
3403.538373	325367.470225	51.361524
3402.877647	325182.450462	51.366529
3402.203166	324998.756414	51.371533
3401.636995	324832.332696	51.376538
3400.994354	324645.119239	51.381543
3400.685358	324462.486483	51.386548
3399.844106	324278.969973	51.391553
3399.311649	324096.117140	51.396557
3398.837754	323887.513520	51.401562
3397.742527	323720.432869	51.406567
3397.204365	323516.014114	51.411572
3396.157047	323347.524787	51.416577
3395.691116	323174.105552	51.421581
3395.252652	322979.854255	51.426586
3394.294456	322799.153775	51.431591
3393.970729	322603.610415	51.436596
3393.052126	322425.907344	51.441601
3392.363139	322229.020514	51.446605
3391.676920	322048.097231	51.451610
3391.068119	321878.338998	51.456615
3390.535068	321687.638936	51.461620
3389.858815	321500.449368	51.466625
3389.308004	321315.887598	51.471629
3388.351782	321136.049073	51.476634
3387.840271	320953.033510	51.481639
3387.479312	320759.783515	51.486644
3386.294523	320584.996038	51.491649
3386.073440	320400.838559	51.496653
3385.308255	320204.239378	51.501658
3384.286372	320021.302634	51.506663
3384.045876	319842.010373	51.511668
3383.006795	319659.330249	51.516673
3382.227157	319471.439882	51.521677
3381.684934	319289.036930	51.526682
3380.935229	319103.661862	51.531687
3380.407670	318919.829971	51.536692
3379.289528	318750.579293	51.541697
3379.016204	318565.637081	51.546701
3378.408296	318383.930245	51.551706
3377.835826	318210.238201	51.556711
3376.899366	318023.897500	51.561716
3376.261437	317836.694420	51.566721
3375.965037	317655.879063	51.571725
3374.974666	317478.839762	51.576730
3374.034571	317297.412566	51.581735
3373.875671	317105.345292	51.586740
3372.770006	316936.802407	51.591745
3372.076756	316759.791206	51.596749
3371.482824	316572.706056	51.601754
3370.551505	316395.655462	51.606759
3370.255425	316223.825906	51.611764
3369.660239	316046.212273	51.616769
3369.232491	315862.969925	51.621773
3368.588054	315688.215337	51.626778
3367.622411	315495.839660	51.631783
3367.198301	315316.542572	51.636788
3366.169019	315140.651122	51.641793
3365.768006	314960.993272	51.646797
3365.319266	314779.993088	51.651802
3364.198616	314603.427656	51.656807
3363.762810	314418.579793	51.661812
3363.056490	314245.716853	51.666817
3362.708093	314051.203783	51.671821
3361.663133	313874.574227	51.676826
3360.611636	313695.271710	51.681831
3360.540232	313510.441023	51.686836
3359.657524	313337.935529	51.691841
3358.848461	313155.843668	51.696845
3358.210909	312973.266026	51.701850
3357.602374	312789.537607	51.706855
3356.872276	312609.953284	51.711860
3356.089485	312431.522884	51.716865
3355.595202	312252.231718	51.721869
3354.744092	312084.786614	51.726874
3353.983715	311909.560318	51.731879
3353.834588	311726.674192	51.736884
3352.728812	311556.696679	51.741889
3351.839463	311377.975875	51.746893
3351.672560	311196.848743	51.751898
3350.829715	311026.370496	51.756903
3350.277646	310852.204591	51.761908
3349.393192	310681.834271	51.766913
3349.018120	310505.780944	51.771917
3348.307619	310320.511287	51.776922
3347.572309	310146.398766	51.781927
3347.082815	309972.501759	51.786932
3346.299085	309791.189871	51.791937
3345.717409	309614.709518	51.796941
3345.131995	309433.824088	51.801946
3344.377963	309254.747589	51.806951
3343.736571	309073.081061	51.811956
3342.959435	308895.662900	51.816961
3342.356298	308704.516830	51.821965
3341.790011	308540.000992	51.826970
3341.121142	308372.292568	51.831975
3340.362778	308182.825463	51.836980
3339.626823	308006.621832	51.841985
3338.897992	307834.109266	51.846989
3338.329140	307648.329288	51.851994
3337.555280	307473.556953	51.856999
3336.828271	307301.450817	51.862004
3335.821300	307128.039068	51.867009
3335.759812	306945.233656	51.872013
3334.978630	306776.547734	51.877018
3334.318192	306600.533941	51.882023
3333.916661	306417.450517	51.887028
3333.173661	306242.544313	51.892033
3332.075059	306061.989855	51.897037
3331.610136	305879.297695	51.902042
3330.866631	305709.585832	51.907047
3330.735331	305525.567150	51.912052
3329.429596	305353.626393	51.917057
3328.891149	305182.277106	51.922061
3328.128739	304996.549464	51.927066
3327.212025	304841.328408	51.932071
3326.699157	304662.080066	51.937076
3325.926390	304487.660161	51.942081
3325.431181	304314.393033	51.947085
3324.948841	304136.106891	51.952090
3324.272725	303969.463599	51.957095
3323.863453	303793.762990	51.962100
3322.943677	303621.835462	51.967105
3322.454625	303444.924682	51.972109
3321.880880	303267.950683	51.977114
3321.130926	303100.554090	51.982119
3320.494758	302906.145319	51.987124
3319.407793	302721.357365	51.992129
3319.058516	302551.706701	51.997133
3318.247139	302383.631432	52.002138
3317.517594	302216.816341	52.007143
3317.225137	302027.165175	52.012148
3316.043471	301858.154710	52.017153
3315.580092	301683.300552	52.022157
3315.051304	301505.604321	52.027162
3314.126458	301338.946502	52.032167
3313.707705	301150.613022	52.037172
3312.934706	300981.715239	52.042177
3312.330235	300814.242207	52.047181
3311.589179	300634.719528	52.052186
3310.969707	300450.338796	52.057191
3310.279394	300280.790542	52.062196
3309.444669	300112.945741	52.067201
3309.070852	299937.107785	52.072205
3308.364602	299752.077868	52.077210
3307.282462	299585.952460	52.082215
3306.794001	299398.188251	52.087220
3306.007718	299252.006998	52.092225
3305.619586	299072.706946	52.097229
3304.827950	298897.519728	52.102234
3304.028741	298731.297808	52.107239
3303.556414	298565.049496	52.112244
3302.974758	298388.886289	52.117249
3302.461205	298219.664564	52.122253
3301.665945	298045.597611	52.127258
3301.133987	297870.291905	52.132263
3300.726464	297685.161614	52.137268
3299.889932	297519.530210	52.142273
3299.056418	297331.716519	52.147277
3298.373757	297170.822775	52.152282
3297.621129	296998.276103	52.157287
3297.263898	296810.590294	52.162292
3296.286141	296645.031389	52.167297
3295.720764	296474.466518	52.172301
3295.303887	296290.329549	52.177306
3293.969500	296127.780785	52.182311
3293.321863	295944.698673	52.187316
3293.190494	295777.884611	52.192321
3292.337268	295610.573375	52.197325
3291.708346	295425.577794	52.202330
3290.710474	295252.813706	52.207335
3290.591347	295076.268675	52.212340
3289.474776	294913.480747	52.217345
3288.967377	294736.920440	52.222349
3288.278464	294569.862511	52.227354
3287.237578	294405.686990	52.232359
3286.920022	294218.349039	52.237364
3286.012813	294056.138556	52.242369
3285.694607	293886.780341	52.247373
3284.953245	293724.976326	52.252378
3283.987903	293550.830483	52.257383
3283.684592	293380.934713	52.262388
3282.585193	293224.942599	52.267393
3282.016174	293038.611192	52.272397
3281.563736	292876.353395	52.277402
3280.730102	292710.946880	52.282407
3280.026093	292539.152877	52.287412
3279.380189	292376.848935	52.292417
3278.975820	292199.659120	52.297421
3278.270785	292033.213095	52.302426
3277.412959	291867.376880	52.307431
3277.008237	291700.170037	52.312436
3276.283144	291525.755498	52.317441
3275.584373	291354.876671	52.322445
3274.833177	291184.795519	52.327450
3273.999597	291025.041677	52.332455
3273.474918	290854.644335	52.337460
3272.876873	290677.764234	52.342465
3272.259588	290506.133402	52.347469
3271.782576	290339.650214	52.352474
3270.708598	290184.314339	52.357479
3270.275507	289997.220619	52.362484
3269.785978	289841.537427	52.367489
3268.884013	289663.405893	52.372493
3268.500633	289490.336708	52.377498
3267.398979	289326.651310	52.382503
3266.826019	289151.447150	52.387508
3266.030361	288988.426262	52.392513
3265.857850	288824.262534	52.397517
3265.042895	288653.374958	52.402522
3264.202957	288493.926306	52.407527
3263.630544	288308.483496	52.412532
3262.749299	288148.098892	52.417537
3262.335425	287975.975981	52.422541
3261.472544	287815.460968	52.427546
3260.762752	287645.065574	52.432551
3260.343622	287479.030068	52.437556
3259.430614	287310.194726	52.442561
3258.624910	287136.681689	52.447565
3258.441272	286978.707502	52.452570
3257.725575	286809.738834	52.457575
3256.995352	286623.785229	52.462580
3256.382905	286477.670334	52.467585
3255.555557	286301.129624	52.472589
3255.310806	286124.420269	52.477594
3254.313292	285954.731747	52.482599
3253.722851	285779.070169	52.487604
3253.116530	285623.072373	52.492609
3252.287166	285456.540545	52.497613
3251.784570	285289.956960	52.502618
3250.827739	285122.833927	52.507623
3250.413566	284944.317146	52.512628
3249.811108	284770.541677	52.517633
3248.856203	284607.442101	52.522637
3248.085714	284446.732766	52.527642
3247.544189	284272.489036	52.532647
3247.293431	284097.995500	52.537652
3246.422421	283948.711625	52.542657
3245.740394	283767.842744	52.547661
3245.307825	283599.617488	52.552666
3244.325923	283438.482827	52.557671
3243.670376	283253.993086	52.562676
3242.455355	283097.632280	52.567681
3241.900190	282935.920594	52.572685
3241.546266	282766.180003	52.577690
3240.664394	282605.742375	52.582695
3240.295106	282426.580867	52.587700
3239.781270	282275.228024	52.592705
3239.008677	282107.107031	52.597709
3238.605970	281935.820350	52.602714
3237.657154	281778.729431	52.607719
3237.153557	281596.787416	52.612724
3236.221252	281432.308003	52.617729
3235.474128	281267.773788	52.622733
3234.746794	281108.482871	52.627738
3234.127801	280942.909579	52.632743
3233.982591	280777.108491	52.637748
3232.907368	280627.321243	52.642753
3232.388285	280449.379910	52.647757
3231.575988	280285.517965	52.652762
3230.677761	280117.900270	52.657767
3230.140202	279961.049525	52.662772
3229.592843	279792.637682	52.667777
3228.828689	279624.412913	52.672781
3228.248102	279452.899128	52.677786
3227.403226	279290.646665	52.682791
3226.757530	279128.490008	52.687796
3226.169408	278980.357282	52.692801
3225.832404	278809.594379	52.697805
3225.334548	278639.162518	52.702810
3224.080585	278479.827113	52.707815
3223.860624	278305.938485	52.712820
3222.881765	278131.660524	52.717825
3222.173692	277974.123363	52.722829
3221.651967	277810.953663	52.727834
3220.995323	277651.600080	52.732839
3220.432713	277490.015858	52.737844
3219.503017	277335.620842	52.742849
3218.971846	277159.743858	52.747853
3218.030972	276999.034428	52.752858
3217.663540	276841.086729	52.757863
3217.126488	276666.585934	52.762868
3216.201119	276500.016294	52.767873
3215.531569	276345.172573	52.772877
3214.849941	276173.419744	52.777882
3214.166709	276021.710789	52.782887
3213.947693	275855.233128	52.787892
3213.077880	275689.418725	52.792897
3212.218258	275520.750248	52.797901
3211.467762	275369.739572	52.802906
3210.759232	275211.743917	52.807911
3210.109462	275054.019119	52.812916
3209.506079	274900.845827	52.817921
3209.006233	274725.371316	52.822925
3208.273240	274564.221461	52.827930
3207.292287	274420.352940	52.832935
3206.542637	274244.841561	52.837940
3205.883572	274091.804445	52.842945
3205.463317	273938.500341	52.847949
3205.022464	273768.619585	52.852954
3204.239222	273611.960162	52.857959
3203.828261	273455.904032	52.862964
3203.081537	273294.858293	52.867969
3202.359181	273120.794372	52.872973
3201.824114	272966.668043	52.877978
3200.952940	272811.856320	52.882983
3200.461219	272632.305729	52.887988
3199.329195	272486.041743	52.892993
3198.740699	272322.347827	52.897997
3198.386818	272162.207851	52.903002
3197.649050	272016.569188	52.908007
3197.111891	271841.126299	52.913012
3196.124263	271682.360069	52.918017
3195.748468	271513.309726	52.923021
3195.234119	271352.991504	52.928026
3194.205855	271197.975623	52.933031
3194.135321	271034.836656	52.938036
3193.197448	270868.625929	52.943041
3192.537059	270704.510671	52.948045
3191.592457	270536.569225	52.953050
3190.665042	270392.896399	52.958055
3190.217136	270214.307085	52.963060
3189.422007	270063.864286	52.968065
3188.770326	269899.162043	52.973069
3188.237495	269743.635086	52.978074
3187.346526	269591.934132	52.983079
3186.635171	269438.447481	52.988084
3186.054049	269284.430895	52.993089
3185.512588	269126.282210	52.998093
3185.050241	268970.234912	53.003098
3184.342930	268801.212129	53.008103
3183.846002	268638.472233	53.013108
3182.724142	268478.301674	53.018113
3182.225610	268323.661019	53.023117
3181.750300	268165.272902	53.028122
3180.944054	268005.358158	53.033127
3180.326046	267841.262359	53.038132
3179.738860	267683.910809	53.043137
3179.013637	267525.103990	53.048141
3178.367137	267363.330453	53.053146
3177.376557	267211.161977	53.058151
3177.107092	267046.450984	53.063156
3175.969318	266895.401026	53.068161
3175.626661	266740.379622	53.073165
3174.903327	266583.151833	53.078170
3174.195610	266430.556828	53.083175
3173.363746	266271.818228	53.088180
3172.969217	266104.249455	53.093185
3172.226090	265963.833977	53.098189
3171.970893	265795.759383	53.103194
3171.131622	265639.467124	53.108199
3170.428404	265475.691248	53.113204
3169.743158	265316.751527	53.118209
3168.984863	265166.660847	53.123213
3168.503517	264998.647828	53.128218
3167.483816	264845.466058	53.133223
3167.036988	264686.769017	53.138228
3166.404583	264532.660181	53.143233
3165.482731	264374.573258	53.148237
3164.869852	264218.551361	53.153242
3164.017027	264071.557697	53.158247
3163.579782	263907.791343	53.163252
3162.944789	263751.976890	53.168257
3162.206379	263595.083748	53.173261
3161.889934	263436.875983	53.178266
3160.832155	263293.073101	53.183271
3160.253860	263132.461986	53.188276
3159.380819	262975.921515	53.193281
3158.745287	262815.930841	53.198285
3158.235911	262670.971807	53.203290
3157.449815	262510.317474	53.208295
3156.856187	262347.824551	53.213300
3156.242711	262207.237205	53.218305
3155.474246	262051.317338	53.223309
3154.856926	261895.195362	53.228314
3154.093954	261754.224393	53.233319
3153.591041	261593.220118	53.238324
3152.634119	261439.393280	53.243329
3152.440231	261284.732693	53.248333
3151.548047	261134.028309	53.253338
3150.939143	260985.927828	53.258343
3150.293790	260823.291116	53.263348
3149.343486	260678.963104	53.268353
3148.789224	260520.998216	53.273357
3148.078753	260371.564344	53.278362
3147.245103	260220.214501	53.283367
3146.760312	260072.655161	53.288372
3146.464355	259924.964153	53.293377
3145.840175	259767.367317	53.298381
3144.653969	259609.070009	53.303386
3144.239238	259457.195902	53.308391
3143.494036	259308.888702	53.313396
3142.687626	259160.311131	53.318401
3142.315316	259002.623977	53.323405
3141.958586	258843.330002	53.328410
3140.885470	258685.320990	53.333415
3140.281596	258537.857784	53.338420
3139.496290	258384.362112	53.343425
3138.887410	258231.297036	53.348429
3138.505518	258079.978865	53.353434
3137.321434	257934.288692	53.358439
3136.936905	257777.546566	53.363444
3136.325260	257631.205721	53.368449
3135.628363	257480.803675	53.373453
3135.185041	257321.397087	53.378458
3134.416452	257167.135552	53.383463
3133.770163	257012.345424	53.388468
3132.814692	256866.619761	53.393473
3132.366986	256708.844213	53.398477
3131.581471	256557.005177	53.403482
3130.565145	256412.384540	53.408487
3130.454047	256246.737612	53.413492
3129.465586	256106.416739	53.418497
3128.233543	255959.996902	53.423501
3128.079182	255805.231668	53.428506
3127.655474	255660.772443	53.433511
3127.011538	255504.989813	53.438516
3126.051172	255365.505410	53.443521
3125.624048	255204.238732	53.448525
3124.995378	255059.277555	53.453530
3124.206915	254916.379135	53.458535
3123.892568	254759.577176	53.463540
3123.013654	254616.744219	53.468545
3122.303440	254465.276815	53.473549
3121.665779	254316.370215	53.478554
3120.663766	254160.874501	53.483559
3120.089990	254011.958027	53.488564
3119.471931	253861.647995	53.493569
3118.884347	253719.839214	53.498573
3118.440124	253566.929749	53.503578
3117.634422	253415.656556	53.508583
3117.090743	253256.982098	53.513588
3116.308648	253112.683339	53.518593
3115.602417	252969.696965	53.523597
3115.081778	252814.457266	53.528602
3114.428828	252669.298018	53.533607
3113.719950	252517.144378	53.538612
3112.722840	252364.374342	53.543617
3112.116029	252210.906009	53.548621
3111.654635	252067.092143	53.553626
3111.036880	251923.303139	53.558631
3110.619980	251772.402739	53.563636
3110.114286	251627.857713	53.568641
3109.087814	251468.726451	53.573645
3108.404278	251315.296518	53.578650
3107.672871	251161.517767	53.583655
3107.011107	251010.300258	53.588660
3106.355147	250861.603151	53.593665
3105.877214	250712.725207	53.598669
3105.288800	250554.060287	53.603674
3104.600138	250416.599471	53.608679
3104.101694	250257.971534	53.613684
3103.315194	250105.399406	53.618689
3102.324436	249949.421785	53.623693
3101.437148	249799.412535	53.628698
3100.734974	249656.071777	53.633703
3100.247172	249502.077775	53.638708
3099.522773	249361.007304	53.643713
3099.278471	249206.262001	53.648717
3098.350071	249051.981638	53.653722
3097.366243	248918.235964	53.658727
3097.260666	248760.642404	53.663732
3096.385360	248616.413218	53.668737
3095.780361	248459.077265	53.673741
3095.262203	248315.301169	53.678746
3094.592113	248158.587016	53.683751
3093.892109	248012.649903	53.688756
3092.975283	247857.859600	53.693761
3092.402683	247713.659776	53.698765
3092.183392	247553.717136	53.703770
3090.802811	247408.015653	53.708775
3089.902411	247257.272470	53.713780
3089.395841	247119.225538	53.718785
3088.656209	246974.951013	53.723789
3088.005765	246827.479288	53.728794
3087.436357	246691.047060	53.733799
3086.517960	246535.570840	53.738804
3085.934529	246414.114989	53.743809
3085.569636	246271.258890	53.748813
3085.090587	246119.813587	53.753818
3084.223074	245985.899394	53.758823
3083.592480	245832.262870	53.763828
3083.064677	245688.108936	53.768833
3082.436433	245552.909481	53.773837
3081.725853	245399.235169	53.778842
3081.105926	245258.355862	53.783847
3080.639728	245105.687295	53.788852
3079.639462	244965.657917	53.793857
3078.654125	244816.840731	53.798861
3078.098417	244674.169290	53.803866
3077.508582	244534.839375	53.808871
3076.941180	244385.396292	53.813876
3076.515091	244239.827216	53.818881
3075.694885	244095.262892	53.823885
3074.896701	243950.007680	53.828890
3074.061887	243810.004276	53.833895
3073.733282	243668.138344	53.838900
3073.090340	243521.993226	53.843905
3072.394738	243380.262088	53.848909
3072.088987	243223.877866	53.853914
3071.101594	243089.578132	53.858919
3070.276612	242943.513418	53.863924
3069.807388	242792.987112	53.868929
3068.808577	242650.260711	53.873933
3068.455721	242493.655666	53.878938
3067.530264	242363.548638	53.883943
3067.029551	242217.407992	53.888948
3066.571838	242083.382024	53.893953
3065.711068	241936.942185	53.898957
3065.026396	241777.462101	53.903962
3064.289828	241645.110499	53.908967
3063.773252	241490.366116	53.913972
3063.054812	241345.636074	53.918977
3062.356220	241205.384862	53.923981
3061.934948	241061.397541	53.928986
3060.943625	240925.012697	53.933991
3060.377929	240775.624600	53.938996
3059.952054	240637.368072	53.944001
3059.233536	240496.560632	53.949005
3058.466168	240344.352966	53.954010
3057.812278	240204.248658	53.959015
3056.890123	240058.584786	53.964020
3056.441385	239926.724310	53.969025
3055.943372	239775.315091	53.974029
3055.202687	239625.421413	53.979034
3054.578110	239484.269303	53.984039
3053.965850	239325.086662	53.989044
3053.114576	239193.290742	53.994049
3052.533075	239052.208746	53.999053
3052.053498	238904.922983	54.004058
3051.170837	238762.921374	54.009063
3050.797479	238617.376210	54.014068
3050.017947	238470.494993	54.019073
3049.257254	238318.314455	54.024077
3048.656243	238176.676447	54.029082
3047.577506	238038.500950	54.034087
3047.369169	237881.599139	54.039092
3046.912022	237743.070998	54.044097
3046.091928	237597.394180	54.049101
3045.329071	237437.856133	54.054106
3044.556537	237298.640025	54.059111
3043.933244	237149.978857	54.064116
3043.043001	237003.855598	54.069121
3042.478793	236855.491055	54.074125
3041.936237	236715.144369	54.079130
3040.957002	236572.626178	54.084135
3040.808724	236424.603829	54.089140
3040.064873	236277.770888	54.094145
3039.020970	236140.941910	54.099149
3038.341761	235994.150065	54.104154
3037.683562	235853.211714	54.109159
3036.894989	235714.509514	54.114164
3036.359679	235584.577773	54.119169
3035.667215	235436.541111	54.124173
3034.913407	235296.051536	54.129178
3034.167423	235160.042466	54.134183
3033.822818	235018.750070	54.139188
3032.886594	234877.729754	54.144193
3032.097843	234747.508174	54.149197
3031.491233	234607.581912	54.154202
3030.767704	234469.609554	54.159207
3030.129252	234329.586869	54.164212
3029.517117	234200.560280	54.169217
3028.973529	234061.872503	54.174221
3028.504305	233924.802785	54.179226
3027.793026	233792.787782	54.184231
3027.448238	233655.571429	54.189236
3026.623028	233512.829464	54.194241
3025.695021	233363.840107	54.199245
3025.205389	233224.432015	54.204250
3024.578791	233087.846714	54.209255
3024.160630	232936.231035	54.214260
3023.106151	232803.074949	54.219265
3022.658578	232657.728201	54.224269
3022.194693	232503.192234	54.229274
3021.150446	232377.164669	54.234279
3020.688313	232231.286162	54.239284
3020.100301	232092.786481	54.244289
3019.331485	231948.815719	54.249293
3018.767020	231806.671593	54.254298
3017.848806	231661.146246	54.259303
3017.349722	231514.765451	54.264308
3016.519808	231371.721895	54.269313
3015.659436	231235.278122	54.274317
3015.188471	231091.516163	54.279322
3014.303387	230957.368318	54.284327
3013.896190	230813.061994	54.289332
3013.200080	230675.778261	54.294337
3012.477663	230535.036049	54.299341
3011.935172	230402.973610	54.304346
3010.762493	230265.103917	54.309351
3010.417032	230118.319104	54.314356
3009.937253	229987.316750	54.319361
3009.260959	229842.647172	54.324365
3008.866425	229702.414522	54.329370
3007.930122	229565.577888	54.334375
3007.154165	229416.850878	54.339380
3006.691235	229284.828416	54.344385
3005.913403	229142.722224	54.349389
3005.443864	229008.791590	54.354394
3004.604824	228868.401464	54.359399
3003.942461	228720.879807	54.364404
3003.112877	228588.152579	54.369409
3002.243773	228452.529193	54.374413
3002.071140	228315.777317	54.379418
3001.085392	228188.014948	54.384423
3000.617499	228042.831575	54.389428
2999.913180	227896.132727	54.394433
2998.982808	227756.064394	54.399437
2998.819841	227615.976663	54.404442
2997.873896	227486.961435	54.409447
2997.441646	227349.946654	54.414452
2996.662277	227212.146822	54.419457
2996.023597	227077.151128	54.424461
2995.709805	226928.915384	54.429466
2994.648776	226793.503239	54.434471
2994.125995	226655.561856	54.439476
2993.371503	226514.003732	54.444481
2992.776081	226381.293796	54.449485
2991.673792	226236.239401	54.454490
2991.112115	226100.125546	54.459495
2990.756736	225967.212780	54.464500
2990.046402	225830.346348	54.469505
2989.349950	225697.564388	54.474509
2988.936604	225547.653727	54.479514
2988.367092	225411.504061	54.484519
2987.638445	225264.113510	54.489524
2986.988556	225118.556647	54.494529
2986.308158	224986.588039	54.499533
2985.654526	224834.157950	54.504538
2984.895349	224696.015403	54.509543
2984.404808	224557.003108	54.514548
2983.578172	224418.133367	54.519553
2982.921032	224278.575070	54.524557
2982.185665	224132.002382	54.529562
2981.231798	224003.261207	54.534567
2980.188987	223863.662848	54.539572
2979.928339	223728.511005	54.544577
2979.175362	223588.561731	54.549581
2978.586798	223453.105827	54.554586
2977.998496	223329.183473	54.559591
2977.452173	223183.091821	54.564596
2976.643857	223038.505856	54.569601
2976.336632	222902.382604	54.574605
2975.761538	222761.604667	54.579610
2974.990894	222622.729230	54.584615
2974.061717	222484.910255	54.589620
2973.553795	222355.986632	54.594625
2972.507011	222209.326817	54.599629
2972.120346	222074.325092	54.604634
2971.172751	221938.712264	54.609639
2970.468222	221793.857609	54.614644
2969.876416	221669.658419	54.619649
2969.164920	221541.022992	54.624653
2968.954160	221401.882926	54.629658
2967.942995	221276.006804	54.634663
2967.251167	221137.045217	54.639668
2966.429949	220996.424064	54.644673
2966.331627	220868.952946	54.649677
2965.650794	220740.963239	54.654682
2964.816487	220599.479296	54.659687
2964.173503	220456.208663	54.664692
2963.160266	220314.702669	54.669697
2962.535804	220182.924347	54.674701
2962.247010	220041.533324	54.679706
2961.387785	219914.617097	54.684711
2960.611487	219768.759375	54.689716
2960.058984	219648.477977	54.694721
2959.388001	219510.012584	54.699725
2958.828651	219374.381147	54.704730
2958.169671	219239.707702	54.709735
2957.453357	219113.457625	54.714740
2957.048239	218983.276086	54.719745
2956.159748	218842.389655	54.724749
2955.920449	218693.190401	54.729754
2954.981318	218558.753512	54.734759
2954.251615	218418.301025	54.739764
2953.574958	218285.974321	54.744769
2952.578779	218143.235132	54.749773
2951.896794	218008.325781	54.754778
2951.227403	217880.071984	54.759783
2950.564925	217741.977790	54.764788
2949.929164	217609.849536	54.769793
2949.145194	217492.676079	54.774797
2948.759771	217360.941445	54.779802
2948.012499	217221.436052	54.784807
2947.314655	217090.515121	54.789812
2946.627430	216961.082033	54.794817
2946.271095	216831.100376	54.799821
2945.462412	216699.319434	54.804826
2944.967009	216573.586246	54.809831
2944.044636	216432.086273	54.814836
2943.742297	216292.474118	54.819841
2943.188923	216163.594121	54.824845
2942.567372	216015.644826	54.829850
2941.279304	215886.690729	54.834855
2941.111375	215739.230278	54.839860
2940.060444	215621.873129	54.844865
2939.250598	215489.407343	54.849869
2939.172054	215345.204844	54.854874
2938.094039	215219.960958	54.859879
2937.428914	215084.736410	54.864884
2936.838545	214949.831239	54.869889
2936.058210	214818.494929	54.874893
2935.430760	214682.679712	54.879898
2934.838679	214561.051372	54.884903
2934.415051	214418.254698	54.889908
2933.734879	214282.015874	54.894913
2932.927714	214143.671798	54.899917
2932.553677	214011.089013	54.904922
2931.519123	213887.851811	54.909927
2930.684666	213740.055767	54.914932
2930.081900	213614.574180	54.919937
2929.487002	213481.569203	54.924941
2928.791472	213353.582610	54.929946
2928.098158	213231.030847	54.934951
2927.173603	213091.778402	54.939956
2926.590742	212968.165936	54.944961
2925.488236	212844.432324	54.949965
2925.617244	212705.790317	54.954970
2924.329158	212588.425155	54.959975
2923.960345	212461.775942	54.964980
2923.559676	212335.081107	54.969985
2922.804662	212211.942815	54.974989
2922.309131	212083.417935	54.979994
2921.552400	211949.716215	54.984999
2920.912966	211822.767446	54.990004
2920.279060	211676.153487	54.995009
2919.573449	211554.739624	55.000013
2919.216884	211426.499527	55.005018
2918.214142	211290.368936	55.010023
2917.615758	211154.581907	55.015028
2916.939854	211024.573108	55.020033
2916.014913	210894.820375	55.025037
2915.610313	210765.341903	55.030042
2914.872731	210639.709259	55.035047
2913.833386	210512.037309	55.040052
2913.546332	210382.655562	55.045057
2912.773278	210251.810988	55.050061
2912.611109	210120.806333	55.055066
2911.910927	209997.510925	55.060071
2911.088004	209862.564069	55.065076
2910.216975	209723.972336	55.070081
2909.731314	209601.280124	55.075085
2909.079303	209462.743391	55.080090
2908.028857	209332.517404	55.085095
2907.655259	209198.773594	55.090100
2907.206833	209077.400173	55.095105
2906.016708	208952.428046	55.100109
2905.686379	208814.618205	55.105114
2904.704738	208691.229968	55.110119
2904.028371	208558.897307	55.115124
2903.621988	208425.287647	55.120129
2902.945938	208303.149987	55.125133
2902.135885	208176.401104	55.130138
2901.550436	208045.607877	55.135143
2900.958893	207911.506852	55.140148
2900.228170	207784.402597	55.145153
2899.272723	207660.286867	55.150157
2898.629745	207528.854789	55.155162
2898.207156	207410.420549	55.160167
2897.809347	207279.535641	55.165172
2896.890930	207158.940456	55.170177
2895.944791	207031.426461	55.175181
2895.629008	206899.854871	55.180186
2894.658848	206783.659415	55.185191
2893.895466	206643.364999	55.190196
2893.718008	206525.542772	55.195201
2892.683997	206405.743753	55.200205
2892.009281	206282.935482	55.205210
2891.534302	206154.839703	55.210215
2890.838228	206022.999378	55.215220
2890.245721	205899.224389	55.220225
2889.701151	205776.842001	55.225229
2889.110649	205650.038279	55.230234
2888.165750	205526.383506	55.235239
2887.857696	205395.055856	55.240244
2887.284471	205260.907016	55.245249
2886.343090	205143.233972	55.250253
2885.745249	205006.875205	55.255258
2885.149547	204882.962888	55.260263
2884.287089	204757.387733	55.265268
2883.802231	204627.375184	55.270273
2882.993280	204496.014344	55.275277
2882.523059	204365.160129	55.280282
2881.458769	204246.846606	55.285287
2880.736019	204106.590044	55.290292
2880.140081	203996.245892	55.295297
2879.393789	203873.479507	55.300301
2878.832947	203743.213744	55.305306
2878.038630	203622.975292	55.310311
2877.460395	203494.609052	55.315316
2876.958900	203374.795628	55.320321
2876.247181	203246.718334	55.325325
2875.803409	203118.484370	55.330330
2874.943122	203006.656872	55.335335
2874.412480	202880.842424	55.340340
2873.434751	202755.671718	55.345345
2872.753816	202634.297533	55.350349
2872.643705	202494.151577	55.355354
2871.657694	202375.905931	55.360359
2871.103805	202249.587546	55.365364
2870.216955	202136.035277	55.370369
2869.738007	202007.822150	55.375373
2869.424344	201875.040045	55.380378
2868.133453	201742.107577	55.385383
2867.977108	201621.848755	55.390388
2867.260638	201494.781563	55.395393
2866.386021	201369.635828	55.400397
2865.817191	201242.787627	55.405402
2864.995487	201125.918454	55.410407
2864.401127	200988.843498	55.415412
2863.759067	200870.737495	55.420417
2862.901709	200745.819511	55.425421
2862.740778	200619.353557	55.430426
2861.647700	200502.897727	55.435431
2861.320327	200368.976141	55.440436
2860.536387	200240.090084	55.445441
2859.725017	200117.024170	55.450445
2859.317141	199988.435474	55.455450
2858.525901	199860.594955	55.460455
2858.017700	199725.354711	55.465460
2857.080202	199607.158262	55.470465
2856.317045	199485.078725	55.475469
2855.974152	199348.986112	55.480474
2855.044195	199230.674772	55.485479
2854.341707	199106.372314	55.490484
2853.953231	198967.233858	55.495489
2853.152620	198858.663011	55.500493
2852.575049	198729.480674	55.505498
2851.684941	198604.763720	55.510503
2850.934015	198478.001747	55.515508
2850.350039	198363.556843	55.520513
2849.423208	198243.083965	55.525517
2849.216514	198110.739527	55.530522
2848.266452	197994.750057	55.535527
2847.826401	197871.706872	55.540532
2847.130915	197743.130960	55.545537
2846.327979	197624.981242	55.550541
2845.621667	197492.755649	55.555546
2844.863416	197385.300904	55.560551
2844.272464	197254.508264	55.565556
2843.845176	197149.775577	55.570561
2842.785161	197033.016721	55.575565
2842.763413	196893.876568	55.580570
2841.707610	196785.172272	55.585575
2840.806349	196657.407821	55.590580
2840.307680	196539.199662	55.595585
2839.648789	196416.067322	55.600589
2839.381042	196307.913636	55.605594
2837.651171	196184.684231	55.610599
2837.573685	196061.028042	55.615604
2836.929766	195946.585214	55.620609
2836.353521	195830.566832	55.625613
2836.045352	195701.527472	55.630618
2834.939411	195587.362200	55.635623
2834.515913	195457.501918	55.640628
2834.127702	195341.900217	55.645633
2833.503250	195217.429263	55.650637
2832.694119	195097.517655	55.655642
2832.029539	194969.274591	55.660647
2831.387219	194838.661646	55.665652
2830.787872	194720.066464	55.670657
2829.869632	194606.866152	55.675661
2829.379282	194472.361985	55.680666
2828.609777	194348.883161	55.685671
2828.064899	194224.274812	55.690676
2826.974117	194100.414863	55.695681
2826.413033	193976.547681	55.700685
2825.826042	193864.976136	55.705690
2825.132157	193747.963253	55.710695
2824.645773	193616.259993	55.715700
2824.183477	193497.595103	55.720705
2823.172627	193373.686130	55.725709
2822.620661	193242.299614	55.730714
2821.965419	193132.598176	55.735719
2821.271021	193010.128665	55.740724
2820.375151	192886.966118	55.745729
2819.762363	192778.162119	55.750733
2819.365063	192649.450080	55.755738
2818.439121	192527.985422	55.760743
2817.468655	192409.416342	55.765748
2816.984702	192294.142214	55.770753
2816.334838	192187.622888	55.775757
2816.183694	192064.013658	55.780762
2815.233576	191948.496083	55.785767
2814.466404	191822.872944	55.790772
2813.658153	191709.343753	55.795777
2812.976515	191585.794298	55.800781
2812.766874	191457.411927	55.805786
2812.015795	191356.330538	55.810791
2811.396016	191227.466629	55.815796
2810.898747	191101.688104	55.820801
2809.964356	190994.376725	55.825805
2809.268644	190863.973593	55.830810
2808.839767	190748.681684	55.835815
2807.973393	190614.820143	55.840820
2807.147512	190506.754734	55.845825
2806.367530	190386.201099	55.850829
2805.725761	190270.638702	55.855834
2805.154550	190159.136731	55.860839
2804.637506	190029.509112	55.865844
2804.042784	189904.741537	55.870849
2803.057810	189790.774115	55.875853
2802.781727	189673.450399	55.880858
2802.097796	189557.858239	55.885863
2801.254421	189433.105835	55.890868
2800.377639	189313.842512	55.895873
2799.851457	189201.228786	55.900877
2799.396066	189081.657583	55.905882
2798.578988	188966.609580	55.910887
2797.796553	188837.319869	55.915892
2797.423584	188728.906883	55.920897
2796.210965	188617.675512	55.925901
2795.825181	188494.837826	55.930906
2795.159868	188382.438929	55.935911
2794.548653	188265.807909	55.940916
2794.140215	188146.587876	55.945921
2793.543616	188028.504787	55.950925
2792.818894	187906.472941	55.955930
2792.398349	187790.563526	55.960935
2791.853320	187666.442848	55.965940
2791.346282	187544.313866	55.970945
2790.174226	187419.351714	55.975949
2789.514607	187287.718695	55.980954
2788.601925	187165.311460	55.985959
2787.945095	187050.777134	55.990964
2787.471155	186938.071539	55.995969
2786.589215	186820.507435	56.000973
2786.341294	186700.069836	56.005978
2785.351829	186581.213014	56.010983
2784.856069	186472.125039	56.015988
2784.385687	186340.884580	56.020993
2783.515822	186229.502893	56.025997
2782.948587	186098.978168	56.031002
2782.375740	185989.496456	56.036007
2781.678649	185862.682278	56.041012
2781.188683	185729.169495	56.046017
2780.402585	185616.885524	56.051021
2779.934255	185473.790675	56.056026
2779.013258	185367.851319	56.061031
2778.151018	185251.242260	56.066036
2777.814579	185122.681069	56.071041
2776.976930	185007.684375	56.076045
2776.306013	184875.105995	56.081050
2775.667542	184755.422358	56.086055
2774.938216	184629.876162	56.091060
2774.351317	184523.567845	56.096065
2773.793909	184400.157689	56.101069
2772.790069	184271.272113	56.106074
2772.119314	184154.152167	56.111079
2771.442484	184034.336600	56.116084
2771.012850	183911.009328	56.121089
2770.372611	183794.674206	56.126093
2769.584109	183666.710357	56.131098
2768.658645	183563.269312	56.136103
2768.111984	183444.299750	56.141108
2767.670090	183326.407919	56.146113
2767.001684	183202.013709	56.151117
2766.227222	183080.384365	56.156122
2765.523262	182962.242432	56.161127
2764.823704	182858.118494	56.166132
2764.155066	182728.459226	56.171137
2763.512512	182618.195396	56.176141
2763.299992	182491.835591	56.181146
2761.893636	182381.985908	56.186151
2761.335533	182254.078714	56.191156
2760.695616	182145.482066	56.196161
2760.351497	182029.893383	56.201165
2760.048037	181910.355188	56.206170
2759.335359	181794.825503	56.211175
2758.292550	181678.788712	56.216180
2757.850673	181553.409267	56.221185
2756.961647	181426.854404	56.226189
2756.216186	181310.262686	56.231194
2755.653137	181203.678759	56.236199
2754.963031	181085.946765	56.241204
2754.421613	180962.263883	56.246209
2753.593989	180842.977017	56.251213
2753.006353	180719.772800	56.256218
2752.203541	180603.637284	56.261223
2751.500708	180485.794466	56.266228
2751.130048	180364.719328	56.271233
2750.779042	180251.464272	56.276237
2750.240091	180130.340131	56.281242
2749.201951	180014.866768	56.286247
2748.744055	179880.603441	56.291252
2748.116664	179756.263496	56.296257
2747.098111	179641.843797	56.301261
2746.541772	179513.880854	56.306266
2746.108557	179396.125538	56.311271
2745.178046	179280.548083	56.316276
2744.567406	179152.162359	56.321281
2743.765136	179033.410767	56.326285
2743.311311	178906.171165	56.331290
2742.425613	178794.785438	56.336295
2741.693694	178675.985551	56.341300
2741.017018	178551.186327	56.346305
2740.254626	178444.106654	56.351309
2739.798358	178319.336805	56.356314
2739.299621	178197.512252	56.361319
2738.555858	178085.406354	56.366324
2738.217194	177957.273744	56.371329
2737.302021	177832.959614	56.376333
2736.454994	177708.787694	56.381338
2735.536848	177594.637487	56.386343
2734.831804	177477.159552	56.391348
2734.637776	177361.725116	56.396353
2733.727390	177249.622421	56.401357
2733.307636	177123.451255	56.406362
2732.408312	177012.771994	56.411367
2731.631025	176888.871300	56.416372
2731.126324	176775.510039	56.421377
2730.335605	176667.587250	56.426381
2730.056361	176538.432085	56.431386
2729.156633	176421.509464	56.436391
2728.463040	176312.427519	56.441396
2727.761709	176193.146564	56.446401
2727.334914	176079.558658	56.451405
2726.748742	175943.687567	56.456410
2726.037556	175834.342586	56.461415
2725.452227	175708.481797	56.466420
2724.774405	175585.561339	56.471425
2723.822575	175473.711709	56.476429
2723.176431	175344.783766	56.481434
2722.618052	175237.629216	56.486439
2721.773318	175108.886101	56.491444
2721.642963	174993.499107	56.496449
2720.505542	174884.097011	56.501453
2719.913664	174753.165555	56.506458
2719.185363	174647.260449	56.511463
2718.649804	174523.099712	56.516468
2718.247294	174409.105637	56.521473
2717.206741	174294.564321	56.526477
2717.075700	174157.673244	56.531482
2716.025544	174045.169075	56.536487
2715.402139	173923.198912	56.541492
2714.895970	173805.280344	56.546497
2714.414327	173687.790652	56.551501
2713.760238	173558.449980	56.556506
2712.465443	173438.902326	56.561511
2711.984734	173325.025463	56.566516
2711.423826	173206.748511	56.571521
2710.482130	173087.845463	56.576525
2710.007030	172968.614503	56.581530
2709.172788	172847.914655	56.586535
2708.589802	172729.909693	56.591540
2708.212313	172606.874463	56.596545
2707.605664	172497.165901	56.601549
2706.980067	172375.455179	56.606554
2706.198363	172261.629047	56.611559
2705.560137	172136.512742	56.616564
2704.939224	172009.600919	56.621569
2704.091171	171894.845259	56.626573
2703.696678	171765.024204	56.631578
2702.923097	171656.463562	56.636583
2701.753126	171537.130803	56.641588
2701.353673	171410.452900	56.646593
2700.647657	171305.405232	56.651597
2700.065533	171188.663767	56.656602
2699.423987	171070.507734	56.661607
2698.727972	170948.443793	56.666612
2698.375105	170831.374585	56.671617
2697.478988	170710.589369	56.676621
2697.193017	170592.391177	56.681626
2696.284779	170470.565828	56.686631
2695.782754	170345.242924	56.691636
2695.311434	170219.127111	56.696641
2694.646507	170096.348775	56.701645
2693.609446	169967.423948	56.706650
2693.083489	169852.699585	56.711655
2692.255983	169730.113488	56.716660
2691.792825	169603.553305	56.721665
2690.888830	169492.272557	56.726669
2690.222807	169365.554544	56.731674
2689.673498	169247.402184	56.736679
2688.956660	169124.406274	56.741684
2688.484188	169001.957009	56.746689
2687.673451	168889.086388	56.751693
2687.359098	168761.945883	56.756698
2686.578195	168644.595062	56.761703
2685.945559	168516.183289	56.766708
2685.255563	168383.241300	56.771713
2684.180165	168266.803009	56.776717
2684.110008	168147.980482	56.781722
2682.942938	168022.020267	56.786727
2682.269587	167898.957845	56.791732
2682.015785	167777.177269	56.796737
2681.095755	167656.481768	56.801741
2680.208651	167540.397366	56.806746
2679.649170	167417.687238	56.811751
2679.199838	167299.067321	56.816756
2678.497763	167178.224379	56.821761
2677.877062	167056.847583	56.826765
2677.185772	166932.201672	56.831770
2676.574385	166811.752450	56.836775
2675.779252	166682.876737	56.841780
2675.486538	166556.197989	56.846785
2674.788641	166447.220519	56.851789
2674.450234	166314.624317	56.856794
2673.215451	166186.811785	56.861799
2672.719404	166060.103355	56.866804
2671.979358	165936.104269	56.871809
2671.194768	165813.218900	56.876813
2670.500915	165680.617690	56.881818
2669.899404	165564.672197	56.886823
2669.322766	165446.116479	56.891828
2668.548747	165318.513682	56.896833
2667.860522	165196.823047	56.901837
2667.088917	165074.344963	56.906842
2666.423646	164955.461551	56.911847
2665.684748	164828.528790	56.916852
2665.405374	164723.012179	56.921857
2664.472806	164598.336038	56.926861
2663.864276	164483.679276	56.931866
2663.366812	164358.553568	56.936871
2662.727230	164222.070941	56.941876
2662.029586	164099.673396	56.946881
2661.435558	163979.345078	56.951885
2660.833977	163857.314571	56.956890
2659.860934	163742.043999	56.961895
2659.102428	163624.845311	56.966900
2658.772193	163496.224946	56.971905
2657.825117	163374.822952	56.976909
2657.302384	163248.573452	56.981914
2656.503335	163128.331289	56.986919
2656.024663	163011.725974	56.991924
2655.646456	162892.562225	56.996929
2654.868742	162760.048452	57.001933
2654.045781	162635.361672	57.006938
2653.461064	162521.025184	57.011943
2652.864211	162393.773265	57.016948
2652.427698	162265.911538	57.021953
2651.561300	162147.577736	57.026957
2650.821590	162011.373580	57.031962
2650.299275	161885.166927	57.036967
2649.688944	161776.481931	57.041972
2649.207414	161639.831433	57.046977
2648.292296	161512.073648	57.051981
2648.087979	161373.676575	57.056986
2647.038546	161252.831946	57.061991
2646.462185	161117.749565	57.066996
2645.574391	160995.583389	57.072001
2644.850909	160866.780455	57.077005
2644.447174	160738.143462	57.082010
2643.525605	160613.326791	57.087015
2642.911238	160488.271185	57.092020
2642.313163	160364.205097	57.097025
2641.198876	160243.399611	57.102029
2640.933147	160105.411329	57.107034
2640.559788	159992.130111	57.112039
2639.590012	159869.650264	57.117044
2639.110695	159724.704951	57.122049
2638.268374	159611.359411	57.127053
2637.760690	159491.871573	57.132058
2637.209654	159358.559044	57.137063
2636.258971	159237.870938	57.142068
2635.873617	159112.110140	57.147073
2635.026742	158985.037191	57.152077
2634.455802	158845.589360	57.157082
2633.777708	158724.503876	57.162087
2633.101241	158597.201933	57.167092
2632.737464	158466.939666	57.172097
2631.855392	158345.023343	57.177101
2631.039244	158205.871182	57.182106
2630.646093	158073.797114	57.187111
2629.842131	157952.505432	57.192116
2629.323088	157825.244942	57.197121
2628.403005	157705.866707	57.202125
2628.157631	157565.889354	57.207130
2627.211514	157446.528853	57.212135
2626.570705	157314.090126	57.217140
2626.054551	157181.848269	57.222145
2625.395735	157052.286406	57.227149
2624.408745	156927.277185	57.232154
2623.885808	156801.571994	57.237159
2623.154648	156672.086590	57.242164
2622.915948	156545.180493	57.247169
2621.647367	156410.518392	57.252173
2621.284214	156274.988775	57.257178
2620.565826	156147.460994	57.262183
2619.972898	156030.172375	57.267188
2619.040665	155893.628499	57.272193
2618.128322	155772.031189	57.277197
2618.051518	155653.378192	57.282202
2617.552632	155525.080678	57.287207
2616.716290	155384.125379	57.292212
2615.794560	155256.747565	57.297217
2615.064547	155141.250662	57.302221
2614.741190	155016.194157	57.307226
2614.022613	154881.501824	57.312231
2613.517944	154756.360605	57.317236
2613.122731	154613.736976	57.322241
2612.259122	154482.844515	57.327245
2611.498572	154349.800729	57.332250
2610.846508	154229.540558	57.337255
2610.029888	154090.074768	57.342260
2609.709355	153950.747045	57.347265
2609.133329	153829.217855	57.352269
2608.508082	153683.367862	57.357274
2607.540726	153550.728640	57.362279
2606.765234	153419.089136	57.367284
2606.228917	153284.361629	57.372289
2605.521319	153163.160775	57.377293
2605.053285	153024.508545	57.382298
2603.980787	152897.862682	57.387303
2603.725474	152761.148019	57.392308
2602.958010	152628.023219	57.397313
2602.209608	152502.954482	57.402317
2601.554290	152363.292419	57.407322
2600.759298	152239.350594	57.412327
2600.089469	152104.788851	57.417332
2599.682999	151966.779531	57.422337
2598.954368	151838.074996	57.427341
2598.484741	151700.000539	57.432346
2597.581979	151572.888005	57.437351
2596.866239	151437.815144	57.442356
2596.506682	151301.974631	57.447361
2595.590307	151184.245875	57.452365
2595.040284	151035.942586	57.457370
2594.205491	150907.906739	57.462375
2593.662061	150783.422150	57.467380
2592.938918	150669.617435	57.472385
2592.423227	150476.826508	57.477389
2591.755077	150326.651392	57.482394
2590.831953	150194.793986	57.487399
2590.400376	150062.960905	57.492404
2590.233527	149922.443853	57.497409
2589.372494	149799.169937	57.502413
2588.500367	149656.414521	57.507418
2588.032429	149522.733808	57.512423
2587.007337	149380.194494	57.517428
2586.732018	149250.703916	57.522433
2585.993264	149115.555387	57.527437
2585.435192	148967.631398	57.532442
2584.193750	148838.130350	57.537447
2583.528126	148709.860334	57.542452
2583.264515	148572.033423	57.547457
2582.192639	148442.862957	57.552461
2581.992732	148294.885316	57.557466
2581.026931	148168.978071	57.562471
2580.242119	148040.462736	57.567476
2580.011953	147901.413359	57.572481
2579.357568	147764.287293	57.577485
2578.539316	147633.262560	57.582490
2578.205572	147494.078869	57.587495
2577.227439	147375.013989	57.592500
2576.989712	147213.639754	57.597505
2575.797229	147081.431159	57.602509
2575.379192	146957.335483	57.607514
2574.949026	146812.819796	57.612519
2573.944136	146670.505428	57.617524
2573.643789	146532.057755	57.622529
2572.452856	146397.551578	57.627533
2572.049401	146264.522421	57.632538
2571.527885	146127.649262	57.637543
2570.662856	145986.230810	57.642548
2570.285839	145839.436420	57.647553
2569.479819	145708.748143	57.652557
2569.156133	145560.002291	57.657562
2568.326106	145427.527177	57.662567
2567.244873	145282.702336	57.667572
2566.806570	145141.804635	57.672577
2565.584291	145011.718961	57.677581
2565.306867	144865.485205	57.682586
2564.671692	144746.312405	57.687591
2563.948199	144603.899299	57.692596
2563.031443	144478.367562	57.697601
2562.500772	144345.417561	57.702605
2562.135708	144211.844641	57.707610
2561.486043	144072.103529	57.712615
2560.852539	143937.290896	57.717620
2559.981558	143791.245213	57.722625
2559.337665	143657.795115	57.727629
2558.748240	143508.148159	57.732634
2558.313897	143393.840961	57.737639
2557.358761	143265.207017	57.742644
2556.954873	143113.524878	57.747649
2556.426528	142977.721348	57.752653
2555.984763	142849.020501	57.757658
2554.987376	142702.466335	57.762663
2554.595008	142555.867820	57.767668
2553.889684	142410.425076	57.772673
2552.769540	142283.460557	57.777677
2552.275870	142126.435369	57.782682
2551.408956	141994.971944	57.787687
2550.741182	141865.243716	57.792692
2550.242019	141719.682653	57.797697
2549.258235	141593.258483	57.802701
2548.633242	141449.408590	57.807706
2548.237959	141307.263718	57.812711
2547.802743	141167.438350	57.817716
2547.139297	141033.062565	57.822721
2545.909184	140900.759313	57.827725
2545.865307	140753.618728	57.832730
2545.085316	140625.667009	57.837735
2544.471533	140486.139915	57.842740
2543.916854	140337.773610	57.847745
2543.198465	140194.084260	57.852749
2542.438790	140049.766858	57.857754
2542.094349	139916.336540	57.862759
2541.132772	139778.265462	57.867764
2540.577062	139629.610594	57.872769
2539.591378	139507.439099	57.877773
2539.374891	139355.326791	57.882778
2538.326862	139210.017300	57.887783
2537.428001	139067.683306	57.892788
2536.916484	138934.677708	57.897793
2536.234094	138801.572733	57.902797
2536.018360	138661.470157	57.907802
2534.968434	138520.331586	57.912807
2534.213752	138377.914521	57.917812
2533.908672	138228.680615	57.922817
2533.060797	138111.117582	57.927821
2532.850963	137962.085906	57.932826
2532.220000	137810.529969	57.937831
2531.388589	137675.547971	57.942836
2530.879092	137518.879736	57.947841
2529.946508	137378.934952	57.952845
2529.573671	137236.043631	57.957850
2528.633068	137094.500715	57.962855
2527.888200	136944.161500	57.967860
2527.655794	136801.199221	57.972865
2526.637600	136664.015527	57.977869
2525.847762	136508.642119	57.982874
2525.285104	136371.883061	57.987879
2524.523623	136222.350541	57.992884
2524.379100	136083.239852	57.997889
2523.534532	135947.010212	58.002893
2522.911513	135793.507049	58.007898
2521.804283	135659.302176	58.012903
2521.355381	135509.101298	58.017908
2520.916090	135367.487309	58.022913
2519.844566	135231.754323	58.027917
2519.414124	135078.618229	58.032922
2518.938024	134931.486192	58.037927
2517.923921	134791.973256	58.042932
2517.461980	134639.035033	58.047937
2516.789868	134498.669007	58.052941
2516.286510	134356.574697	58.057946
2515.297891	134222.268777	58.062951
2514.777508	134074.081072	58.067956
2514.739341	133919.593251	58.072961
2513.476628	133776.516998	58.077965
2512.802622	133627.797017	58.082970
2512.384921	133491.054012	58.087975
2511.417136	133346.497753	58.092980
2510.799183	133196.056266	58.097985
2510.001031	133052.821089	58.102989
2509.614987	132900.654961	58.107994
2508.634382	132774.306344	58.112999
2508.102186	132622.799986	58.118004
2507.941216	132480.508298	58.123009
2506.811495	132333.683724	58.128013
2506.240773	132188.651239	58.133018
2505.941447	132037.085694	58.138023
2504.997129	131888.328724	58.143028
2504.710217	131747.356284	58.148033
2504.035737	131604.439067	58.153037
2503.348570	131442.598803	58.158042
2502.339179	131294.274439	58.163047
2501.548896	131155.467830	58.168052
2501.306372	130997.916343	58.173057
2500.134923	130846.241384	58.178061
2499.622454	130700.559534	58.183066
2499.043741	130562.687639	58.188071
2498.426787	130413.340416	58.193076
2497.876794	130258.229676	58.198081
2496.812654	130123.510602	58.203085
2496.489219	129968.492573	58.208090
2495.886647	129828.646691	58.213095
2495.051629	129682.640231	58.218100
2494.935789	129537.676341	58.223105
2493.594444	129389.605200	58.228109
2493.154816	129228.665668	58.233114
2492.620328	129083.249765	58.238119
2491.745209	128948.633430	58.243124
2491.149349	128798.656484	58.248129
2490.313159	128650.725137	58.253133
2489.781524	128495.380006	58.258138
2489.369208	128346.240058	58.263143
2488.305314	128211.263519	58.268148
2487.824720	128055.519061	58.273153
2487.032625	127912.105999	58.278157
2486.471949	127759.512871	58.283162
2485.646690	127611.331366	58.288167
2485.089036	127471.680778	58.293172
2484.648369	127319.248875	58.298177
2483.603467	127176.197227	58.303181
2482.973092	127026.679901	58.308186
2482.614338	126877.094942	58.313191
2482.090310	126732.794675	58.318196
2481.460873	126576.866310	58.323201
2480.607535	126430.638695	58.328205
2480.001047	126278.721462	58.333210
2479.353536	126117.680694	58.338215
2478.523267	125982.170147	58.343220
2478.154497	125844.034569	58.348225
2477.198597	125686.905822	58.353229
2476.861085	125528.930720	58.358234
2475.814433	125382.383815	58.363239
2475.330094	125239.278902	58.368244
2474.954825	125094.747875	58.373249
2474.266648	124944.717812	58.378253
2473.680104	124782.646712	58.383258
2472.757231	124630.560296	58.388263
2471.978139	124475.734439	58.393268
2471.402287	124326.870989	58.398273
2470.609456	124184.747571	58.403277
2470.347403	124031.277255	58.408282
2469.720683	123871.960878	58.413287
2468.731625	123719.534563	58.418292
2468.523250	123569.778982	58.423297
2467.388177	123410.380856	58.428301
2466.775451	123258.024504	58.433306
2466.134201	123116.377962	58.438311
2465.666753	122960.876572	58.443316
2465.151006	122808.532815	58.448321
2464.158764	122679.121486	58.453325
2463.650005	122506.195232	58.458330
2463.178284	122359.688021	58.463335
2462.233692	122205.625331	58.468340
2461.756818	122037.547552	58.473345
2460.931404	121877.995262	58.478349
2460.253036	121735.117632	58.483354
2459.630681	121589.908294	58.488359
2458.968149	121429.926582	58.493364
2458.766408	121274.532644	58.498369
2457.797514	121137.963985	58.503373
2457.020222	120964.938020	58.508378
2456.080874	120819.262606	58.513383
2455.359433	120659.790097	58.518388
2454.648771	120501.497647	58.523393
2454.372566	120365.788162	58.528397
2453.362304	120208.801945	58.533402
2452.600262	120052.729565	58.538407
2451.774807	119908.971040	58.543412
2451.542934	119766.122231	58.548417
2450.565396	119622.110075	58.553421
2450.244914	119464.104866	58.558426
2449.681581	119312.703032	58.563431
2448.660009	119169.163775	58.568436
2448.307727	119018.714148	58.573441
2447.457466	118870.699430	58.578445
2447.014498	118716.996720	58.583450
2446.370592	118570.169815	58.588455
2445.413834	118419.121220	58.593460
2445.181377	118262.804258	58.598465
2444.411027	118113.778250	58.603469
2443.598046	117966.213497	58.608474
2442.949694	117813.024806	58.613479
2442.345396	117671.236828	58.618484
2441.628858	117506.971368	58.623489
2440.916546	117353.814595	58.628493
2440.587550	117205.631595	58.633498
2439.872384	117062.436351	58.638503
2439.153374	116890.063088	58.643508
2438.715747	116745.200667	58.648513
2437.877212	116604.534787	58.653517
2437.078999	116430.914041	58.658522
2436.763688	116278.894077	58.663527
2435.794813	116134.449398	58.668532
2434.923759	115978.076215	58.673537
2434.194977	115824.309193	58.678541
2433.828351	115671.291785	58.683546
2433.047051	115512.095440	58.688551
2432.112647	115373.603248	58.693556
2431.868224	115219.217260	58.698561
2431.067949	115071.914761	58.703565
2430.631673	114923.806473	58.708570
2430.107004	114771.485988	58.713575
2429.209544	114602.057098	58.718580
2428.668431	114453.409659	58.723585
2427.789185	114308.282078	58.728589
2427.068826	114140.573600	58.733594
2426.548915	113995.447981	58.738599
2425.548998	113846.286614	58.743604
2425.400040	113686.671519	58.748609
2424.396670	113542.132898	58.753613
2423.544698	113390.107495	58.758618
2423.219434	113236.984066	58.763623
2422.496146	113091.261268	58.768628
2421.996930	112940.439292	58.773633
2421.484364	112778.596545	58.778637
2420.957559	112625.832483	58.783642
2420.457614	112466.750453	58.788647
2419.394864	112311.617233	58.793652
2419.021476	112147.052988	58.798657
2418.362078	112000.196806	58.803661
2417.527084	111829.393319	58.808666
2417.245858	111655.203211	58.813671
2416.240414	111507.040384	58.818676
2415.571689	111348.715739	58.823681
2414.548278	111191.546204	58.828685
2414.150917	111025.831884	58.833690
2413.470061	110882.158749	58.838695
2412.506989	110727.343310	58.843700
2412.011803	110569.237305	58.848705
2411.152651	110420.734178	58.853709
2410.680656	110266.249928	58.858714
2409.849933	110112.185228	58.863719
2409.135373	109957.119493	58.868724
2408.595963	109802.921716	58.873729
2407.893184	109666.893040	58.878733
2407.423460	109502.114247	58.883738
2406.522142	109350.679928	58.888743
2406.032113	109203.553423	58.893748
2405.476155	109037.579439	58.898753
2404.557265	108894.044541	58.903757
2404.218310	108743.013446	58.908762
2403.844101	108579.780373	58.913767
2402.910291	108434.499230	58.918772
2402.489642	108261.643438	58.923777
2401.323276	108114.395970	58.928781
2400.727934	107963.137529	58.933786
2400.204836	107809.286093	58.938791
2399.733912	107658.879118	58.943796
2398.996089	107488.541043	58.948801
2398.358001	107332.077665	58.953805
2397.630420	107178.732200	58.958810
2396.919778	107012.225566	58.963815
2396.514039	106858.063379	58.968820
2395.495238	106699.792717	58.973825
2394.721989	106558.177449	58.978829
2394.205170	106386.733513	58.983834
2393.803152	106233.824670	58.988839
2392.689864	106083.148702	58.993844
2392.178147	105923.362525	58.998849
2391.550893	105776.164457	59.003853
2390.753258	105617.174324	59.008858
2390.119965	105465.391988	59.013863
2389.599366	105305.960302	59.018868
2388.931808	105146.115214	59.023873
2387.964647	104997.186705	59.028877
2387.601386	104847.452816	59.033882
2387.297023	104690.966489	59.038887
2386.227211	104527.002071	59.043892
2385.979212	104358.854514	59.048897
2385.355371	104216.537950	59.053901
2384.776126	104063.518881	59.058906
2383.739852	103900.638342	59.063911
2383.296540	103734.752979	59.068916
2382.886695	103565.025326	59.073921
2381.931064	103412.450795	59.078925
2381.055236	103248.946641	59.083930
2380.816466	103084.333938	59.088935
2379.970810	102931.364458	59.093940
2379.528336	102772.356160	59.098945
2378.689511	102604.676383	59.103949
2377.900448	102439.711382	59.108954
2377.222564	102289.999202	59.113959
2376.392337	102129.312228	59.118964
2375.892620	101956.464000	59.123969
2375.032034	101796.805448	59.128973
2374.643311	101646.360100	59.133978
2374.070396	101493.210883	59.138983
2373.330055	101325.702291	59.143988
2372.793184	101171.058771	59.148993
2372.025037	101013.205150	59.153997
2371.632151	100848.467703	59.159002
2370.699872	100691.270283	59.164007
2370.010969	100514.587027	59.169012
2369.509352	100351.538617	59.174017
2368.559022	100199.225303	59.179021
2367.915225	100037.939666	59.184026
2367.654700	99871.982996	59.189031
2366.596057	99718.865429	59.194036
2366.128715	99547.019527	59.199041
2365.182584	99393.385193	59.204045
2364.783039	99223.161088	59.209050
2364.013358	99069.589743	59.214055
2363.039923	98906.746876	59.219060
2362.826110	98744.380943	59.224065
2362.059918	98591.167442	59.229069
2361.528085	98425.854097	59.234074
2360.757138	98274.235476	59.239079
2359.897770	98115.407706	59.244084
2359.259051	97949.004811	59.249089
2358.523290	97788.453584	59.254093
2357.937621	97621.023533	59.259098
2357.131890	97470.918921	59.264103
2356.353930	97315.603840	59.269108
2355.923850	97146.719244	59.274113
2355.458110	97000.007698	59.279117
2354.669579	96836.363861	59.284122
2354.204670	96676.532266	59.289127
2353.466476	96525.966562	59.294132
2352.470818	96366.322785	59.299137
2352.096659	96203.315451	59.304141
2351.296011	96043.700113	59.309146
2350.709926	95889.455211	59.314151
2349.866682	95728.802437	59.319156
2349.448067	95556.332045	59.324161
2348.656652	95402.744534	59.329165
2348.084942	95252.979024	59.334170
2347.373577	95094.307525	59.339175
2346.534109	94950.458914	59.344180
2346.052195	94768.974066	59.349185
2345.468135	94619.202062	59.354189
2345.070296	94459.007761	59.359194
2344.023601	94305.595075	59.364199
2343.064825	94134.546636	59.369204
2343.122548	93977.479638	59.374209
2342.281544	93822.889864	59.379213
2341.523098	93653.157719	59.384218
2341.185446	93492.992514	59.389223
2340.518347	93331.656846	59.394228
2339.840888	93164.788156	59.399233
2338.940530	93005.222983	59.404237
2338.284403	92845.398295	59.409242
2337.891850	92675.989724	59.414247
2336.617238	92522.593778	59.419252
2336.460242	92349.821338	59.424257
2335.747216	92200.029006	59.429261
2335.123985	92039.735697	59.434266
2334.168714	91869.737721	59.439271
2333.320399	91715.709118	59.444276
2332.971016	91545.256151	59.449281
2332.384949	91384.891966	59.454285
2332.151927	91222.393251	59.459290
2331.494507	91059.595280	59.464295
2330.376444	90896.459426	59.469300
2330.018409	90726.014186	59.474305
2329.261435	90568.548957	59.479309
2328.424533	90400.407670	59.484314
2327.757318	90226.876861	59.489319
2327.048077	90063.314657	59.494324
2326.404209	89900.015943	59.499329
2325.388637	89748.424299	59.504333
2325.066087	89572.333333	59.509338
2324.726880	89415.862638	59.514343
2323.846527	89258.648333	59.519348
2323.366414	89086.466387	59.524353
2322.489276	88924.397563	59.529357
2321.681710	88761.849767	59.534362
2320.949657	88598.562135	59.539367
2320.340032	88435.896641	59.544372
2319.744932	88276.209749	59.549377
2318.791790	88121.297551	59.554381
2318.489468	87958.935601	59.559386
2318.192237	87789.486384	59.564391
2316.997904	87627.198643	59.569396
2316.437259	87469.667708	59.574401
2315.680683	87314.863268	59.579405
2315.305613	87142.211039	59.584410
2314.631553	86986.045588	59.589415
2313.953284	86824.398427	59.594420
2313.297870	86641.867301	59.599425
2312.611820	86498.892982	59.604429
2312.036799	86333.828986	59.609434
2311.599640	86170.341864	59.614439
2310.576519	85999.164521	59.619444
2310.067344	85828.648719	59.624449
2309.466206	85663.834927	59.629453
2308.708186	85505.671468	59.634458
2308.043257	85333.859488	59.639463
2307.190991	85175.504246	59.644468
2306.981206	85002.881122	59.649473
2305.956089	84837.291571	59.654477
2305.312934	84666.235847	59.659482
2304.850881	84501.795671	59.664487
2304.017610	84340.299692	59.669492
2303.717644	84161.327445	59.674497
2303.193054	84002.979712	59.679501
2302.033732	83845.957139	59.684506
2301.472394	83667.119264	59.689511
2300.818655	83497.779699	59.694516
2300.581710	83320.750452	59.699521
2299.554888	83168.446612	59.704525
2298.694364	82991.480993	59.709530
2298.487010	82823.952167	59.714535
2297.844780	82653.438685	59.719540
2297.055300	82477.499241	59.724545
2296.045448	82315.767926	59.729549
2295.457405	82143.722550	59.734554
2294.843738	81981.785219	59.739559
2293.932974	81826.050285	59.744564
2293.750806	81647.226537	59.749569
2292.703600	81474.701763	59.754573
2292.122383	81309.202709	59.759578
2291.575113	81151.589922	59.764583
2290.790942	80978.292386	59.769588
2290.362793	80807.538218	59.774593
2289.531578	80648.713109	59.779597
2288.878977	80455.283962	59.784602
2288.084805	80314.650245	59.789607
2287.352898	80154.609074	59.794612
2287.070259	79973.819402	59.799617
2286.144590	79808.298223	59.804621
2285.337876	79655.478189	59.809626
2284.539593	79483.025574	59.814631
2283.811836	79318.604944	59.819636
2283.324916	79158.900190	59.824641
2282.951096	79005.775517	59.829645
2282.371165	78828.420631	59.834650
2281.717245	78662.656444	59.839655
2280.509329	78495.929543	59.844660
2280.472253	78331.445296	59.849665
2279.685539	78179.602582	59.854669
2278.760562	78007.505614	59.859674
2278.302848	77834.803717	59.864679
2277.441437	77676.291472	59.869684
2276.872444	77508.007552	59.874689
2276.197011	77353.663081	59.879693
2275.779324	77171.525469	59.884698
2275.149219	77012.816951	59.889703
2274.445915	76846.403669	59.894708
2273.858378	76668.783587	59.899713
2273.433916	76513.157448	59.904718
2272.301719	76339.219246	59.909722
2271.616865	76177.966132	59.914727
2270.561673	76001.623575	59.919732
2270.406157	75838.065270	59.924737
2269.503434	75676.692299	59.929742
2268.677713	75516.024360	59.934746
2268.280134	75345.919110	59.939751
2267.501019	75187.064779	59.944756
2267.203932	75011.408942	59.949761
2266.251509	74855.461129	59.954766
2265.734517	74680.894771	59.959770
2265.298014	74518.595486	59.964775
2264.537372	74347.390501	59.969780
2263.785078	74177.902561	59.974785
2262.950060	74017.653525	59.979790
2262.611416	73843.186535	59.984794
2261.896204	73674.964037	59.989799
2260.980479	73520.287840	59.994804
2260.427736	73344.997552	59.999809
2259.880579	73190.588549	60.004814
2258.976582	73018.790481	60.009818
2258.562369	72842.114258	60.014823
2257.386741	72674.904457	60.019828
2257.326447	72516.926544	60.024833
2256.368410	72352.757383	60.029838
2256.019790	72187.200621	60.034842
2255.488600	72017.372882	60.039847
2254.347595	71845.191775	60.044852
2254.108338	71674.364129	60.049857
2253.418905	71510.862481	60.054862
2252.462459	71335.596917	60.059866
2252.187931	71168.282239	60.064871
2251.216633	71003.676609	60.069876
2250.807396	70826.377764	60.074881
2250.035080	70664.277164	60.079886
2249.142767	70490.503836	60.084890
2248.757601	70321.687320	60.089895
2247.912993	70157.417049	60.094900
2247.421453	69986.872044	60.099905
2247.043596	69810.736510	60.104910
2246.038237	69647.249754	60.109914
2245.521992	69470.461483	60.114919
2244.803612	69302.219628	60.119924
2243.883729	69126.594244	60.124929
2243.117885	68962.251821	60.129934
2242.523208	68788.231017	60.134938
2242.273242	68623.068580	60.139943
2241.044451	68468.012918	60.144948
2240.807045	68293.813185	60.149953
2239.901174	68128.214281	60.154958
2239.394391	67960.229106	60.159962
2238.941075	67784.883812	60.164967
2237.891247	67617.735069	60.169972
2237.561916	67440.530212	60.174977
2236.765848	67280.234757	60.179982
2236.414712	67099.876181	60.184986
2235.281541	66931.723763	60.189991
2234.593292	66770.981604	60.194996
2234.295861	66591.645204	60.200001
2233.347170	66429.845245	60.205006
2233.023570	66251.472431	60.210010
2231.944109	66087.492233	60.215015
2231.412428	65923.591202	60.220020
2230.839398	65754.942232	60.225025
2230.226615	65595.980564	60.230030
2229.535019	65416.021021	60.235034
2228.931973	65251.054160	60.240039
2228.157715	65065.921462	60.245044
2227.389115	64897.187558	60.250049
2226.817436	64734.015423	60.255054
2226.645809	64567.551725	60.260058
2225.621537	64398.052232	60.265063
2224.927975	64228.606271	60.270068
2224.443910	64036.297906	60.275073
2223.608445	63871.563434	60.280078
2222.668092	63703.510023	60.285082
2222.371606	63527.795550	60.290087
2221.098294	63360.643302	60.295092
2220.923354	63189.857926	60.300097
2220.403402	63025.121895	60.305102
2219.771402	62856.055128	60.310106
2218.899552	62692.213597	60.315111
2218.201134	62519.582938	60.320116
2217.620814	62337.130617	60.325121
2216.802449	62167.159314	60.330126
2216.003468	62008.386887	60.335130
2215.986385	61825.581074	60.340135
2215.144785	61673.361769	60.345140
2214.499840	61494.628531	60.350145
2213.866185	61317.516002	60.355150
2213.093357	61134.751284	60.360154
2212.537954	60967.006163	60.365159
2211.793585	60797.295051	60.370164
2211.350597	60620.845762	60.375169
2210.367957	60452.751987	60.380174
2209.538793	60281.754806	60.385178
2208.903713	60103.102877	60.390183
2208.299761	59929.081862	60.395188
2207.644329	59758.815267	60.400193
2206.575366	59594.899023	60.405198
2206.420413	59426.328664	60.410202
2205.502444	59255.155544	60.415207
2204.591992	59086.331425	60.420212
2204.089191	58916.947234	60.425217
2203.159107	58756.672174	60.430222
2202.971924	58588.902636	60.435226
2202.439521	58421.331800	60.440231
2201.828831	58251.961283	60.445236
2200.953900	58083.647054	60.450241
2200.195203	57915.800170	60.455246
2199.742297	57748.843150	60.460250
2199.112692	57578.209448	60.465255
2198.311519	57407.981165	60.470260
2197.728914	57240.394157	60.475265
2197.215612	57078.238166	60.480270
2196.523407	56904.522162	60.485274
2195.912622	56730.981606	60.490279
2195.096946	56555.313609	60.495284
2194.236527	56389.424113	60.500289
2193.617612	56221.358421	60.505294
2193.313832	56051.228338	60.510298
2192.481287	55875.569511	60.515303
2191.491177	55712.184671	60.520308
2191.380655	55543.098303	60.525313
2190.771132	55365.820328	60.530318
2189.735004	55190.456696	60.535322
2189.389499	55021.801659	60.540327
2188.727913	54854.176157	60.545332
2187.922793	54678.815601	60.550337
2186.954091	54507.387638	60.555342
2186.418154	54340.307036	60.560346
2186.107100	54169.382339	60.565351
2185.298699	53997.152139	60.570356
2184.379975	53829.886956	60.575361
2183.579238	53652.924928	60.580366
2182.671097	53492.103742	60.585370
2182.602787	53317.101416	60.590375
2181.698424	53169.284464	60.595380
2181.135831	52997.717722	60.600385
2180.802096	52828.122391	60.605390
2180.072575	52648.102278	60.610394
2179.608917	52465.137123	60.615399
2178.399197	52307.165056	60.620404
2178.211602	52123.890619	60.625409
2177.506756	51952.672768	60.630414
2176.736967	51787.538557	60.635418
2176.249245	51609.866608	60.640423
2175.358763	51436.730944	60.645428
2175.266465	51260.037493	60.650433
2174.009598	51091.854672	60.655438
2173.437670	50917.654711	60.660442
2173.084643	50742.399805	60.665447
2171.972791	50564.125351	60.670452
2171.653743	50392.288528	60.675457
2171.013600	50225.401733	60.680462
2169.975654	50048.082471	60.685466
2169.577530	49868.819058	60.690471
2168.597249	49697.713884	60.695476
2168.019144	49513.582130	60.700481
2167.084293	49351.011628	60.705486
2166.729768	49188.666903	60.710490
2166.034522	49012.376020	60.715495
2165.070606	48852.076596	60.720500
2164.537369	48667.358074	60.725505
2163.995221	48496.144339	60.730510
2163.369698	48330.879994	60.735514
2162.594758	48162.474373	60.740519
2161.966107	47991.358321	60.745524
2161.524097	47826.246718	60.750529
2160.906814	47659.747319	60.755534
2160.438454	47471.570359	60.760538
2159.808554	47298.623371	60.765543
2158.894617	47140.023838	60.770548
2158.512139	46957.706421	60.775553
2157.971278	46780.227103	60.780558
2157.190544	46590.723657	60.785562
2156.478210	46417.342917	60.790567
2155.760347	46247.981790	60.795572
2155.021245	46067.147207	60.800577
2154.257871	45901.269599	60.805582
2153.424816	45722.474601	60.810586
2153.045599	45537.745441	60.815591
2152.183112	45379.235883	60.820596
2151.643459	45198.106625	60.825601
2150.939841	45026.544235	60.830606
2150.374012	44859.516048	60.835610
2149.916104	44687.386666	60.840615
2148.961310	44505.372147	60.845620
2148.505044	44325.152739	60.850625
2147.569782	44159.091232	60.855630
2146.688320	43981.374907	60.860634
2146.470905	43802.242584	60.865639
2145.311542	43637.736484	60.870644
2144.710800	43470.018763	60.875649
2144.250889	43304.705942	60.880654
2143.812559	43127.902099	60.885658
2142.779628	42962.082591	60.890663
2141.951065	42794.701655	60.895668
2141.667407	42607.445881	60.900673
2140.768804	42450.160977	60.905678
2139.950853	42269.843221	60.910682
2139.848367	42105.560337	60.915687
2138.896015	41934.324128	60.920692
2138.482804	41752.549867	60.925697
2137.764230	41590.061413	60.930702
2137.218116	41403.872240	60.935706
2136.348000	41239.026900	60.940711
2135.637155	41069.215559	60.945716
2135.173386	40887.363605	60.950721
2134.419415	40720.547521	60.955726
2133.789343	40531.889467	60.960730
2133.433761	40366.970882	60.965735
2132.589474	40195.462952	60.970740
2131.972478	40018.812673	60.975745
2131.194309	39848.162514	60.980750
2130.391643	39667.245221	60.985754
2129.776848	39496.632733	60.990759
2129.009809	39325.355266	60.995764
2128.827832	39146.852289	61.000769
2127.883850	38974.926652	61.005774
2127.432396	38798.167910	61.010778
2126.801311	38611.108926	61.015783
2125.895266	38435.355598	61.020788
2125.312713	38267.687436	61.025793
2124.551256	38088.000770	61.030798
2124.007225	37917.471951	61.035802
2123.512446	37737.794113	61.040807
2122.364141	37570.613054	61.045812
2122.168622	37386.463902	61.050817
2121.650810	37206.782718	61.055822
2120.730086	37038.993871	61.060826
2120.076329	36851.433160	61.065831
2119.158857	36671.255222	61.070836
2118.680072	36489.204557	61.075841
2118.201160	36316.078326	61.080846
2117.282715	36139.269745	61.085850
2116.866183	35957.682810	61.090855
2115.776906	35794.069451	61.095860
2115.265430	35600.471932	61.100865
2114.612456	35442.329366	61.105870
2114.078595	35270.188337	61.110874
2113.623250	35088.822436	61.115879
2112.858119	34912.337540	61.120884
2112.086564	34730.007887	61.125889
2111.415561	34558.061898	61.130894
2110.409080	34391.280377	61.135898
2109.946690	34208.145618	61.140903
2109.143558	34041.270542	61.145908
2108.539345	33861.052614	61.150913
2107.878293	33690.272409	61.155918
2107.122309	33516.824045	61.160922
2106.717576	33343.612539	61.165927
2106.066119	33178.262868	61.170932
2105.468747	32983.965039	61.175937
2104.467764	32829.510272	61.180942
2103.833905	32643.752484	61.185946
2103.270627	32467.019744	61.190951
2102.224697	32310.870306	61.195956
2101.854536	32125.831839	61.200961
2101.041491	31969.079814	61.205966
2100.225788	31792.675614	61.210970
2099.830813	31618.439294	61.215975
2099.331425	31461.514338	61.220980
2098.391781	31289.012841	61.225985
2097.916028	31122.470788	61.230990
2097.385437	30954.238954	61.235994
2097.012253	30767.574517	61.240999
2095.713484	30614.957430	61.246004
2095.612687	30423.919604	61.251009
2094.812881	30261.518926	61.256014
2093.786618	30081.927470	61.261018
2093.267752	29915.910107	61.266023
2092.659741	29736.600516	61.271028
2092.173109	29558.531271	61.276033
2091.338344	29399.890757	61.281038
2090.450318	29238.427443	61.286042
2090.181163	29059.379607	61.291047
2089.188976	28891.182190	61.296052
2088.536159	28715.591019	61.301057
2087.809247	28545.054801	61.306062
2087.266270	28380.707835	61.311066
2086.458668	28218.992261	61.316071
2085.780714	28038.502318	61.321076
2085.327297	27875.610728	61.326081
2084.519967	27701.661676	61.331086
2084.024696	27531.756534	61.336090
2083.448709	27360.109316	61.341095
2082.380658	27192.257494	61.346100
2081.939764	27021.634257	61.351105
2081.151513	26853.722600	61.356110
2080.806548	26678.630681	61.361114
2079.980776	26522.079929	61.366119
2079.185333	26360.099831	61.371124
2078.833154	26188.471415	61.376129
2077.985747	26017.352271	61.381134
2077.234010	25844.647288	61.386138
2077.194012	25671.865974	61.391143
2075.750595	25511.876924	61.396148
2075.234781	25340.128730	61.401153
2074.916873	25167.082616	61.406158
2074.034158	25012.109064	61.411162
2073.582015	24827.424067	61.416167
2072.808814	24653.630460	61.421172
2072.289913	24489.076096	61.426177
2071.525025	24320.778127	61.431182
2070.620659	24143.803041	61.436186
2070.317281	23970.580397	61.441191
2069.084054	23805.129294	61.446196
2068.816324	23647.084778	61.451201
2067.999252	23473.750833	61.456206
2067.501543	23312.649807	61.461210
2066.863577	23139.069979	61.466215
2066.044503	22977.517960	61.471220
2065.583438	22803.290693	61.476225
2064.826435	22630.595231	61.481230
2063.949596	22463.102980	61.486234
2063.275109	22304.381474	61.491239
2062.594729	22126.549984	61.496244
2061.937767	21953.129854	61.501249
2060.985965	21805.769967	61.506254
2060.456703	21622.105602	61.511258
2059.807979	21466.138539	61.516263
2058.977387	21309.652337	61.521268
2058.765742	21142.084314	61.526273
2057.968962	20987.976462	61.531278
2057.112811	20822.251917	61.536282
2056.673038	20650.103331	61.541287
2055.766173	20507.638830	61.546292
2055.285857	20334.609937	61.551297
2054.616051	20171.994303	61.556302
2053.879410	20013.435585	61.561306
2053.500855	19850.756138	61.566311
2052.319529	19682.349350	61.571316
2051.836637	19520.102791	61.576321
2051.119682	19362.279382	61.581326
2050.484144	19210.723244	61.586330
2049.955338	19039.537624	61.591335
2049.029174	18890.877479	61.596340
2048.822800	18724.085972	61.601345
2047.851443	18565.397203	61.606350
2047.076715	18402.922773	61.611354
2046.571253	18240.639394	61.616359
2045.642147	18082.768641	61.621364
2045.009758	17920.882124	61.626369
2044.212606	17768.736094	61.631374
2043.450189	17619.427424	61.636378
2043.184201	17459.483914	61.641383
2042.666854	17309.004215	61.646388
2041.767000	17147.365343	61.651393
2040.967073	17000.705033	61.656398
2040.042705	16830.119947	61.661402
2039.569792	16677.142636	61.666407
2038.606604	16537.976569	61.671412
2038.098951	16384.059882	61.676417
2037.718568	16244.805347	61.681422
2036.668191	16091.339008	61.686426
2035.950478	15944.786558	61.691431
2034.798457	15802.039540	61.696436
2034.305081	15638.357100	61.701441
2033.462947	15509.620729	61.706446
2032.786536	15382.765811	61.711450
2032.068103	15239.833746	61.716455
2031.167854	15099.481349	61.721460
2030.588143	14976.915374	61.726465
2029.504301	14847.458614	61.731470
2028.585934	14717.144043	61.736474
2027.686601	14602.236058	61.741479
2026.549609	14490.421535	61.746484
2026.253571	14376.083757	61.751489
2024.956056	14281.342643	61.756494
2023.943440	14174.881177	61.761498
2023.177795	14073.659634	61.766503
2022.116064	13981.826088	61.771508
2021.294813	13889.488616	61.776513
2020.781079	13808.456053	61.781518
2020.009378	13725.163106	61.786522
2018.995135	13635.558284	61.791527
2018.251959	13557.656824	61.796532
2017.880848	13482.339969	61.801537
2017.086055	13409.763830	61.806542
2016.109851	13332.958600	61.811546
2015.828402	13248.890855	61.816551
2014.761388	13176.993905	61.821556
2014.316619	13109.879545	61.826561
2013.413432	13039.595623	61.831566
2012.599671	12973.999360	61.836570
2012.023374	12911.812072	61.841575
2011.421118	12858.435549	61.846580
2010.903597	12773.859733	61.851585
2010.067119	12730.871122	61.856590
2009.175901	12658.694919	61.861594
2008.904108	12594.909765	61.866599
2007.827715	12544.785822	61.871604
2007.624605	12463.531978	61.876609
2006.716498	12416.348047	61.881614
2005.884467	12349.841017	61.886618
2005.313581	12290.093377	61.891623
2004.310628	12229.657198	61.896628
2003.968278	12173.123485	61.901633
2003.384776	12111.946326	61.906638
2002.676434	12068.617107	61.911642
2002.618911	11990.425494	61.916647
2001.644965	11939.645169	61.921652
2001.060851	11875.674691	61.926657
2000.636888	11811.995291	61.931662
1999.593553	11763.590471	61.936666
1998.794846	11688.397999	61.941671
1998.161578	11639.123242	61.946676
1997.780487	11573.416035	61.951681
1996.886999	11527.857649	61.956686
1996.232792	11468.587682	61.961690
1995.692094	11404.279122	61.966695
1995.038494	11345.344893	61.971700
1994.584680	11284.569484	61.976705
1993.808785	11230.300688	61.981710
1993.065633	11168.783400	61.986714
1992.742132	11102.426020	61.991719
1991.792858	11052.370095	61.996724
1991.271987	10976.113283	62.001729
1990.557047	10927.932427	62.006734
1989.895857	10870.573020	62.011738
1989.413637	10802.413558	62.016743
1988.633369	10749.211591	62.021748
1987.847395	10685.352355	62.026753
1987.055415	10625.618761	62.031758
1986.542728	10579.969269	62.036762
1985.842297	10525.416453	62.041767
1985.016507	10464.609094	62.046772
1984.760283	10407.216370	62.051777
1984.206479	10349.759844	62.056782
1983.599560	10284.340254	62.061786
1983.220829	10218.865795	62.066791
1982.653184	10164.951632	62.071796
1981.666643	10092.995914	62.076801
1980.989418	10035.087570	62.081806
1980.408489	9975.779490	62.086810
1979.963371	9894.436615	62.091815
1978.707481	9846.334428	62.096820
1978.333572	9777.313466	62.101825
1977.709795	9726.267860	62.106830
1976.792446	9662.885700	62.111834
1976.393998	9598.668774	62.116839
1975.517458	9558.170561	62.121844
1974.762661	9498.268283	62.126849
1974.369167	9443.991783	62.131854
1973.686271	9374.183839	62.136858
1973.026223	9310.243591	62.141863
1972.157057	9256.740308	62.146868
1971.468097	9193.646564	62.151873
1970.855930	9137.516350	62.156878
1970.218945	9078.514199	62.161882
1969.863540	9014.504769	62.166887
1969.023758	8960.729246	62.171892
1968.382785	8890.967784	62.176897
1967.627306	8843.371235	62.181902
1967.346675	8782.537414	62.186906
1966.744890	8724.409145	62.191911
1965.557762	8665.105425	62.196916
1965.002702	8614.663322	62.201921
1964.145227	8547.886007	62.206926
1963.676163	8501.048203	62.211930
1963.049025	8422.820921	62.216935
1962.214070	8382.972508	62.221940
1961.794903	8323.441751	62.226945
1961.069389	8263.507027	62.231950
1960.367144	8210.046869	62.236954
1959.955677	8144.462799	62.241959
1958.925929	8092.777985	62.246964
1958.629449	8035.438187	62.251969
1957.940881	7969.371103	62.256974
1957.125426	7922.446123	62.261978
1956.575620	7866.588468	62.266983
1956.146885	7800.411469	62.271988
1955.538766	7747.601471	62.276993
1954.577900	7686.256083	62.281998
1953.625991	7625.047578	62.287002
1953.282808	7561.898344	62.292007
1952.096465	7515.290686	62.297012
1952.035548	7450.399496	62.302017
1951.654565	7402.185650	62.307022
1950.930406	7336.549056	62.312026
1950.103345	7283.612954	62.317031
1949.250138	7220.484592	62.322036
1948.555246	7155.358479	62.327041
1947.783683	7099.306193	62.332046
1947.174595	7045.534882	62.337050
1946.970677	6981.871401	62.342055
1945.934944	6931.315661	62.347060
1945.360979	6862.945326	62.352065
1944.710423	6800.416064	62.357070
1943.863529	6762.022957	62.362074
1942.966895	6705.603912	62.367079
1942.811436	6642.623617	62.372084
1942.180166	6589.497993	62.377089
1941.377390	6528.492779	62.382094
1940.715515	6458.860391	62.387098
1940.373284	6406.154149	62.392103
1939.442887	6345.512285	62.397108
1938.474764	6290.985081	62.402113
1937.951379	6238.181984	62.407118
1937.671857	6175.151584	62.412122
1937.162250	6118.289200	62.417127
1936.058311	6062.856784	62.422132
1935.522897	5997.163813	62.427137
1934.586109	5941.277013	62.432142
1933.987219	5891.451358	62.437146
1933.513794	5822.128855	62.442151
1932.580696	5774.370374	62.447156
1931.928407	5725.150063	62.452161
1931.730116	5658.606062	62.457166
1931.194229	5608.600198	62.462170
1930.378700	5542.740743	62.467175
1929.603861	5479.987536	62.472180
1928.925101	5419.222764	62.477185
1928.028654	5370.148086	62.482190
1927.432340	5314.598464	62.487194
1927.122982	5247.006775	62.492199
1926.541573	5198.765257	62.497204
1925.599048	5138.595626	62.502209
1924.928030	5079.828883	62.507214
1924.263724	5019.613996	62.512218
1923.387813	4950.679692	62.517223
1922.639203	4911.752085	62.522228
1921.930701	4859.376870	62.527233
1921.491683	4806.472427	62.532238
1920.671896	4758.988709	62.537242
1920.351640	4695.483653	62.542247
1919.739597	4650.125218	62.547252
1918.819263	4585.667701	62.552257
1918.254279	4528.781580	62.557262
1917.612750	4469.595368	62.562266
1917.159304	4410.560937	62.567271
1916.231257	4367.778147	62.572276
1915.856345	4288.743929	62.577281
1915.113494	4246.760215	62.582286
1914.120642	4183.909905	62.587290
1913.709535	4126.731970	62.592295
1912.659436	4077.801143	62.597300
1911.896910	4022.079302	62.602305
1911.553083	3965.687874	62.607310
1910.915586	3925.343775	62.612314
1910.295100	3866.700043	62.617319
1909.351247	3809.966754	62.622324
1908.907133	3753.648055	62.627329
1908.386902	3699.986807	62.632334
1907.405630	3650.171074	62.637338
1907.126213	3592.073672	62.642343
1906.243795	3546.870400	62.647348
1905.381379	3483.197177	62.652353
1904.886747	3441.815956	62.657358
1904.182472	3386.918511	62.662362
1903.565302	3325.790623	62.667367
1902.854634	3273.120940	62.672372
1902.214527	3224.347121	62.677377
1901.720495	3172.738027	62.682382
1901.067812	3126.841867	62.687386
1900.781963	3063.572619	62.692391
1899.849599	3013.191370	62.697396
1899.301882	2963.885629	62.702401
1898.159302	2897.772133	62.707406
1897.545008	2842.289124	62.712410
1897.460991	2794.411068	62.717415
1896.599343	2737.134213	62.722420
1896.217516	2684.233068	62.727425
1895.155714	2620.256943	62.732430
1894.495660	2568.774911	62.737434
1894.082530	2504.180577	62.742439
1892.906144	2455.748384	62.747444
1892.213413	2403.377074	62.752449
1891.583359	2348.787968	62.757454
1890.989983	2290.291346	62.762458
1890.469713	2244.270480	62.767463
1889.779394	2196.356574	62.772468
1889.537914	2144.328559	62.777473
1888.680210	2078.042649	62.782478
1887.795556	2035.795238	62.787482
1887.342917	1976.326521	62.792487
1886.575109	1913.898147	62.797492
1885.971438	1866.678119	62.802497
1885.043292	1809.445431	62.807502
1884.045521	1749.418356	62.812506
1883.828068	1701.457031	62.817511
1882.691272	1656.038205	62.822516
1882.562443	1597.034550	62.827521
1881.626907	1560.992181	62.832526
1880.757562	1503.090568	62.837530
1880.391223	1459.782393	62.842535
1879.387460	1421.335130	62.847540
1879.139711	1363.899978	62.852545
1878.336340	1327.422442	62.857550
1877.654290	1278.903866	62.862554
1877.305700	1214.940548	62.867559
1876.474037	1175.914649	62.872564
1875.675071	1118.473353	62.877569
1875.301876	1070.639761	62.882574
1874.039090	1019.566418	62.887578
1873.843940	974.559289	62.892583
1872.773429	930.281074	62.897588
1872.344968	872.846588	62.902593
1871.451461	837.333954	62.907598
1870.685091	795.273234	62.912602
1870.497746	737.826234	62.917607
1869.420525	698.154616	62.922612
1868.847207	661.076095	62.927617
1868.145776	609.016200	62.932622
1867.307515	565.761960	62.937626
1867.177034	521.734730	62.942631
1866.225296	467.467901	62.947636
1865.751422	434.691900	62.952641
1865.055623	389.058015	62.957646
1864.206347	354.433681	62.962650
1863.434174	300.695634	62.967655
1862.537289	269.147799	62.972660
1861.888047	213.359458	62.977665
1861.500943	178.573861	62.982670
1860.714924	133.391918	62.987674
1860.042322	94.966570	62.992679
1859.016908	62.800940	62.997684
1858.477898	30.436735	63.002689
1857.550380	1.794299	63.007694
1856.771005	-26.660293	63.012698
1856.168643	-56.984760	63.017703
1855.151544	-85.524492	63.022708
1853.568115	-87.302534	63.027713
1848.445640	27.092425	63.032718
1848.483445	19.944611	63.037722
1849.425029	24.155324	63.042727
1849.976984	26.980291	63.047732
1849.897306	11.167061	63.052737
1849.748256	11.484069	63.057742
1848.710947	23.590773	63.062746
1848.333984	3.363659	63.067751
1847.059016	30.242784	63.072756
1846.865045	15.248771	63.077761
1846.421317	19.655773	63.082766
1845.330160	28.767009	63.087770
1844.772843	20.489996	63.092775
1843.714818	22.351623	63.097780
1842.685134	19.859619	63.102785
1842.228104	27.020453	63.107790
1841.699660	28.523616	63.112794
1841.981758	23.305004	63.117799
1841.176707	31.396284	63.122804
1840.546965	32.084496	63.127809
1839.760850	33.273764	63.132814
1838.703340	31.923135	63.137818
1838.329334	23.434094	63.142823
1837.342964	35.013918	63.147828
1836.649439	30.331820	63.152833
1836.187698	29.727096	63.157838
1835.343304	29.662509	63.162842
1834.857548	33.719807	63.167847
1833.803596	42.588611	63.172852
1833.226015	25.887772	63.177857
1833.266157	25.146593	63.182862
1832.359949	31.043101	63.187866
1832.120298	21.834158	63.192871
1830.526405	36.922888	63.197876
1830.400587	25.089226	63.202881
1830.210744	28.140775	63.207886
1828.940275	35.383461	63.212890
1828.050294	25.445162	63.217895
1827.855349	20.677599	63.222900
1827.345289	26.758783	63.227905
1826.636893	19.798834	63.232910
1825.460693	36.055970	63.237914
1825.091108	32.120360	63.242919
1824.670224	44.321597	63.247924
1823.874850	39.766055	63.252929
1822.794360	31.732956	63.257934
1822.412619	26.318555	63.262938
1822.151180	27.129638	63.267943
1821.410651	32.813767	63.272948
1820.352226	22.481182	63.277953
1819.589089	32.573225	63.282958
1819.221247	29.130915	63.287962
1819.116685	25.544303	63.292967
1817.355585	32.298783	63.297972
1817.302876	26.664986	63.302977
1817.014034	33.551545	63.307982
1815.499479	33.818872	63.312986
1815.024771	23.727911	63.317991
1814.541822	34.835154	63.322996
1814.334598	32.527952	63.328001
1813.306063	29.242588	63.333006
1812.162985	36.537592	63.338010
1812.259612	24.230231	63.343015
1811.149052	30.789958	63.348020
1810.400393	28.349536	63.353025
1810.327548	15.285365	63.358030
1809.271467	38.851355	63.363034
1808.715482	30.017484	63.368039
1808.016363	27.182853	63.373044
1807.200553	26.986007	63.378049
1806.883610	32.315881	63.383054
1806.038937	31.694697	63.388058
1805.927902	23.624368	63.393063
1805.147558	28.179443	63.398068
1804.224847	27.007692	63.403073
1804.166452	24.399323	63.408078
1802.939120	36.302839	63.413082
1801.738187	30.616403	63.418087
1801.002863	37.905012	63.423092
1801.122472	29.331290	63.428097
1800.405186	31.686019	63.433102
1799.125171	29.538126	63.438106
1798.446763	28.362277	63.443111
1798.140447	32.547202	63.448116
1798.014408	29.804497	63.453121
1797.327830	33.549921	63.458126
1796.614036	25.668342	63.463130
1795.979917	24.580076	63.468135
1795.327755	37.773642	63.473140
1793.874379	34.640899	63.478145
1793.492036	34.613340	63.483150
1792.445775	32.915599	63.488154
1792.669114	24.525678	63.493159
1791.461100	32.810262	63.498164
1790.526857	24.366040	63.503169
1790.232407	32.368368	63.508174
1789.645009	34.547937	63.513178
1789.084052	30.879261	63.518183
1788.593164	27.402881	63.523188
1788.094167	39.324788	63.528193
1787.765741	28.530953	63.533198
1786.442020	43.644615	63.538202
1785.437288	28.858191	63.543207
1784.484974	34.173846	63.548212
1784.551429	19.665178	63.553217
1783.892544	25.710077	63.558222
1783.035068	37.854483	63.563226
1782.799302	27.243051	63.568231
1781.817714	29.672869	63.573236
1781.206468	27.614326	63.578241
1780.814598	32.743217	63.583246
1779.913487	27.070685	63.588250
1778.990845	35.373037	63.593255
1777.882493	30.274294	63.598260
1777.371556	25.517492	63.603265
1777.764069	30.677941	63.608270
1776.503065	34.241780	63.613274
1776.136189	27.019460	63.618279
1775.516984	31.460647	63.623284
1774.917803	21.736387	63.628289
1773.829725	22.038515	63.633294
1772.814812	38.363093	63.638298
1772.518985	25.495174	63.643303
1771.367457	31.167310	63.648308
1771.156875	14.766191	63.653313
1770.790289	28.892089	63.658318
1769.991180	30.457169	63.663322
1769.742237	22.430822	63.668327
1769.097303	21.744817	63.673332
1768.252493	21.675588	63.678337
1767.261770	28.771373	63.683342
1766.505933	20.770330	63.688346
1766.043405	20.462203	63.693351
1765.382617	30.142196	63.698356
1764.914026	24.722676	63.703361
1764.448970	25.143485	63.708366
1763.231215	33.005438	63.713370
1762.568205	26.793642	63.718375
1761.532683	34.667657	63.723380
1760.961186	21.020373	63.728385
1760.515634	25.489177	63.733390
1759.915823	28.631063	63.738394
1759.696717	23.307541	63.743399
1759.009192	25.037827	63.748404
1758.543523	24.552009	63.753409
1757.966276	32.072558	63.758414
1756.823337	34.236279	63.763418
1755.921946	24.247786	63.768423
1755.504306	24.378800	63.773428
1754.804068	20.531985	63.778433
1754.545109	22.749286	63.783438
1753.243538	32.128928	63.788442
1752.556283	34.120941	63.793447
1751.681994	24.148646	63.798452
1751.370702	28.564593	63.803457
1750.770899	23.047646	63.808462
1749.977345	30.047472	63.813466
1749.380127	18.137308	63.818471
1748.910251	22.829166	63.823476
1748.822384	23.874458	63.828481
1748.198715	19.714295	63.833486
1747.050065	32.516787	63.838490
1746.384605	24.537666	63.843495
1745.739680	35.814137	63.848500
1744.904320	32.829275	63.853505
1744.602577	19.691079	63.858510
1743.123598	26.299875	63.863514
1742.674576	25.541764	63.868519
1742.031698	30.631675	63.873524
1741.301587	28.625134	63.878529
1741.185415	27.796817	63.883534
1740.531625	26.426268	63.888538
1740.264386	25.063716	63.893543
1739.044145	30.169626	63.898548
1738.332566	28.086028	63.903553
1738.006444	28.902660	63.908558
1737.312282	32.767570	63.913562
1736.637301	31.201696	63.918567
1735.390494	30.598668	63.923572
1734.404581	23.294902	63.928577
1733.925995	16.389951	63.933582
1733.361839	35.312661	63.938586
1733.268552	27.176445	63.943591
1732.474083	25.142282	63.948596
1732.264894	29.103633	63.953601
1731.932707	23.588344	63.958606
1730.154132	32.975943	63.963610
1729.851845	30.657039	63.968615
1729.123216	32.718705	63.973620
1728.703759	32.615051	63.978625
1728.073748	23.280468	63.983630
1726.671399	30.301294	63.988634
1726.328573	33.465451	63.993639
1725.398088	34.906333	63.998644
1724.959645	26.908511	64.003649
1724.521988	27.667166	64.008654
1723.797272	36.273981	64.013658
1723.772263	29.759027	64.018663
1722.668905	38.269864	64.023668
1721.730358	29.583508	64.028673
1721.162357	30.780747	64.033678
1720.349010	30.720728	64.038682
1720.007871	27.622694	64.043687
1719.493470	31.542635	64.048692
1718.239596	30.686855	64.053697
1717.738651	33.499243	64.058702
1716.794691	34.929653	64.063706
1716.556015	26.412839	64.068711
1716.104739	32.927817	64.073716
1715.345635	30.918004	64.078721
1715.092723	40.865960	64.083726
1714.162167	25.121649	64.088730
1713.062657	28.536868	64.093735
1712.633874	37.041493	64.098740
1712.323912	28.383041	64.103745
1711.389725	24.384164	64.108750
1709.987693	29.933687	64.113754
1709.551053	29.843804	64.118759
1709.013251	33.846309	64.123764
1708.586520	23.719375	64.128769
1708.258056	19.487108	64.133774
1707.747945	25.673968	64.138778
1707.483616	27.455322	64.143783
1706.052361	30.100083	64.148788
1705.581842	30.389310	64.153793
1704.986232	28.763531	64.158798
1703.976713	30.820931	64.163802
1702.829568	23.240019	64.168807
1702.038037	30.067651	64.173812
1701.606708	28.183975	64.178817
1701.368089	19.621429	64.183822
1700.674110	29.076472	64.188826
1700.425553	24.385247	64.193831
1699.850648	29.336639	64.198836
1699.144406	25.683177	64.203841
1697.981798	25.429485	64.208846
1697.463772	26.883713	64.213850
1696.804938	24.761789	64.218855
1696.307690	35.141200	64.223860
1695.685140	32.127287	64.228865
1694.853224	26.861681	64.233870
1693.872390	22.860760	64.238874
1693.512651	23.181278	64.243879
1692.999364	23.072033	64.248884
1692.274188	31.377734	64.253889
1691.392411	29.593988	64.258894
1690.417957	30.258140	64.263898
1690.050112	33.549274	64.268903
1689.596419	30.180545	64.273908
1688.875111	40.731163	64.278913
1688.689652	36.805756	64.283918
1687.457461	30.238119	64.288922
1687.078312	22.079508	64.293927
1686.220058	30.694921	64.298932
1685.855107	24.647117	64.303937
1685.247986	18.834894	64.308942
1683.980715	20.717201	64.313946
1683.653404	22.905942	64.318951
1682.882880	36.599276	64.323956
1682.633428	20.262694	64.328961
1681.906198	26.788387	64.333966
1680.754282	31.060321	64.338970
1680.196662	26.101229	64.343975
1679.444408	27.058089	64.348980
1679.148857	17.186292	64.353985
1678.871719	14.218447	64.358990
1677.697694	26.545604	64.363994
1677.230910	25.049177	64.368999
1676.602697	20.801449	64.374004
1675.599674	29.484013	64.379009
1674.761067	25.216086	64.384014
1673.838801	23.421433	64.389018
1673.624091	12.264232	64.394023
1672.797753	27.954910	64.399028
1672.627032	20.375039	64.404033
1672.463168	17.941121	64.409038
1671.225101	18.008501	64.414042
1670.591908	12.025389	64.419047
1670.029463	30.596170	64.424052
1669.339256	22.140050	64.429057
1668.076132	19.820813	64.434062
1667.081413	27.199529	64.439066
1667.172962	16.854675	64.444071
1666.192561	23.677620	64.449076
1665.928874	28.333586	64.454081
1665.497628	18.413961	64.459086
1664.289089	27.275823	64.464090
1664.082095	26.823049	64.469095
1663.226546	27.201826	64.474100
1662.877824	19.025773	64.479105
1661.884763	27.053915	64.484110
1660.351673	22.513118	64.489114
1660.438586	11.730622	64.494119
1659.871237	27.850083	64.499124
1659.356857	26.476335	64.504129
1659.143168	18.157413	64.509134
1658.161797	32.127082	64.514138
1657.104921	20.075502	64.519143
1656.426964	21.118336	64.524148
1656.010326	22.665273	64.529153
1655.376041	14.089895	64.534158
1653.750752	32.534622	64.539162
1653.384665	15.910658	64.544167
1653.093149	22.999487	64.549172
1652.803027	28.599492	64.554177
1652.396499	20.437354	64.559182
1651.485416	27.395947	64.564186
1650.525876	21.417368	64.569191
1649.782591	21.451895	64.574196
1649.289481	22.703483	64.579201
1649.295936	26.945964	64.584206
1648.065342	19.728413	64.589210
1647.050405	25.643819	64.594215
1646.307828	19.663894	64.599220
1646.082545	22.728963	64.604225
1645.583651	24.686349	64.609230
1644.675358	29.350095	64.614234
1643.698747	24.454415	64.619239
1643.399628	19.482657	64.624244
1642.637169	33.094290	64.629249
1642.127199	25.757539	64.634254
1641.691365	22.280333	64.639258
1640.916722	20.815471	64.644263
1640.253273	19.876980	64.649268
1639.704891	26.017890	64.654273
1638.490466	22.388403	64.659278
1637.408217	16.700553	64.664282
1636.973233	20.035469	64.669287
1636.479426	36.080182	64.674292
1636.150150	28.364653	64.679297
1635.825001	16.882810	64.684302
1635.336198	29.700362	64.689306
1634.453053	17.484008	64.694311
1633.259097	25.777453	64.699316
1632.794270	16.569629	64.704321
1632.212596	17.904671	64.709326
1631.565815	25.944045	64.714330
1630.917688	17.388218	64.719335
1629.765368	24.768326	64.724340
1629.522824	21.720876	64.729345
1629.191081	20.253469	64.734350
1627.982507	26.533946	64.739354
1627.398209	15.722461	64.744359
1627.060918	23.912938	64.749364
1626.287320	23.471329	64.754369
1625.867926	14.420290	64.759374
1625.093298	21.762478	64.764378
1624.612884	16.955137	64.769383
1623.809443	18.263911	64.774388
1622.273419	23.148802	64.779393
1621.823162	19.877313	64.784398
1621.295777	25.374664	64.789402
1621.055457	23.328200	64.794407
1619.922413	22.125277	64.799412
1619.742427	20.606956	64.804417
1619.356806	29.990952	64.809422
1618.227305	20.954947	64.814426
1617.765992	20.165697	64.819431
1617.045391	23.987524	64.824436
1616.059356	18.754318	64.829441
1615.342484	13.213436	64.834446
1614.658433	24.415706	64.839450
1614.142140	16.874973	64.844455
1613.630273	21.888901	64.849460
1613.326955	23.378420	64.854465
1613.108802	18.825879	64.859470
1611.556149	25.477981	64.864474
1611.358013	16.070106	64.869479
1610.540298	24.835208	64.874484
1609.515009	30.695503	64.879489
1608.873189	12.118991	64.884494
1608.253529	21.466047	64.889498
1607.777289	24.088451	64.894503
1607.259264	25.422849	64.899508
1606.223890	18.026079	64.904513
1605.568617	10.538969	64.909518
1604.588930	23.762497	64.914522
1604.589939	25.692513	64.919527
1604.429562	21.824634	64.924532
1602.912296	20.969755	64.929537
1602.152002	24.797892	64.934542
1601.624007	17.046139	64.939546
1601.455394	19.450943	64.944551
1600.781980	25.818297	64.949556
1599.558079	32.088607	64.954561
1599.304599	27.057565	64.959566
1598.809234	22.057068	64.964570
1597.852092	22.310083	64.969575
1596.935563	21.906959	64.974580
1596.111963	20.460927	64.979585
1595.826747	25.014662	64.984590
1595.326701	29.610413	64.989594
1594.832938	28.414748	64.994599
1593.841143	19.102998	64.999604
1593.059043	27.474527	65.004609
1592.664337	15.328829	65.009614
1591.832200	16.919706	65.014618
1591.473887	31.001712	65.019623
1590.194593	14.497619	65.024628
1589.495895	31.929443	65.029633
1589.406071	13.109130	65.034638
1588.575848	29.839622	65.039642
1588.510631	19.076566	65.044647
1587.056414	26.052079	65.049652
1586.478846	27.042712	65.054657
1586.191133	22.367187	65.059662
1585.172013	31.571139	65.064666
1584.237611	22.354350	65.069671
1583.577531	14.232514	65.074676
1583.203898	25.475357	65.079681
1583.105893	24.026014	65.084686
1582.220302	25.335236	65.089690
1581.399441	17.387172	65.094695
1580.150019	24.077846	65.099700
1579.841244	29.597242	65.104705
1579.757559	11.424069	65.109710
1578.986931	27.372406	65.114714
1578.260824	15.618398	65.119719
1577.348352	18.578185	65.124724
1576.893216	14.225722	65.129729
1575.484487	30.710668	65.134734
1574.431942	14.291983	65.139738
1574.574415	9.921846	65.144743
1573.934751	13.787591	65.149748
1572.890524	20.800471	65.154753
1573.107503	5.386439	65.159758
1572.297806	23.454038	65.164762
1571.979302	8.344268	65.169767
1570.748597	30.272806	65.174772
1569.917687	11.570240	65.179777
1569.516638	20.314881	65.184782
1568.561390	24.833148	65.189786
1567.679701	19.127658	65.194791
1567.150566	23.858916	65.199796
1566.959301	28.976454	65.204801
1566.611052	18.591096	65.209806
1565.481768	22.293367	65.214810
1564.854213	15.948278	65.219815
1564.242217	15.838972	65.224820
1563.517503	12.026069	65.229825
1563.101242	14.662603	65.234830
1562.072623	25.471783	65.239834
1561.391042	14.693123	65.244839
1560.946107	20.421802	65.249844
1560.364533	31.992571	65.254849
1559.532776	28.952012	65.259854
1558.652404	23.200584	65.264858
1558.214169	16.927917	65.269863
1557.656583	31.910460	65.274868
1557.088545	15.540959	65.279873
1556.052289	18.119885	65.284878
1555.278002	28.631625	65.289882
1555.156697	22.776944	65.294887
1554.385499	18.059974	65.299892
1553.555479	30.447631	65.304897
1552.918433	11.864079	65.309902
1552.274960	28.479751	65.314906
1551.993128	21.832159	65.319911
1551.029527	23.663127	65.324916
1550.119586	15.606231	65.329921
1549.592278	18.290372	65.334926
1549.009083	26.800614	65.339930
1548.852884	16.078828	65.344935
1547.652598	22.646593	65.349940
1546.956084	15.355282	65.354945
1546.668130	14.273580	65.359950
1544.814550	16.674873	65.364954
1544.533159	10.001987	65.369959
1543.584094	27.760587	65.374964
1543.497158	15.793077	65.379969
1543.069365	21.709841	65.384974
1542.399250	17.295351	65.389978
1542.392397	21.202481	65.394983
1541.195289	26.763677	65.399988
1540.325794	19.608657	65.404993
1540.119170	18.871992	65.409998
1539.009830	20.620468	65.415002
1538.068629	13.481576	65.420007
1537.570117	20.409336	65.425012
1537.471382	27.566886	65.430017
1537.207978	16.013758	65.435022
1535.475491	22.625088	65.440026
1534.831416	16.681591	65.445031
1534.272010	25.869279	65.450036
1534.069218	20.581045	65.455041
1533.308789	25.180329	65.460046
1532.027696	34.564691	65.465050
1531.646444	20.305384	65.470055
1531.131418	28.077842	65.475060
1530.581894	34.110146	65.480065
1529.810120	18.676594	65.485070
1528.866656	23.754380	65.490074
1528.648098	24.984442	65.495079
1527.984066	21.390558	65.500084
1527.334305	17.906368	65.505089
1526.756943	28.271709	65.510094
1525.963290	28.017816	65.515098
1525.704830	23.908493	65.520103
1524.187001	25.822803	65.525108
1523.305364	14.877255	65.530113
1523.129829	22.945842	65.535118
1522.577939	25.160822	65.540122
1522.419543	23.402542	65.545127
1521.167305	30.189881	65.550132
1520.270780	24.450497	65.555137
1519.969460	17.632550	65.560142
1519.210536	21.307528	65.565146
1519.099812	4.436471	65.570151
1518.003960	24.487565	65.575156
1517.141159	22.929519	65.580161
1516.817030	27.092062	65.585166
1515.415788	28.177320	65.590170
1515.203944	15.542130	65.595175
1514.474391	17.588227	65.600180
1513.979844	27.945140	65.605185
1513.790587	14.610945	65.610190
1512.349330	28.576449	65.615194
1511.581335	16.882738	65.620199
1511.125784	29.624050	65.625204
1510.422444	23.641090	65.630209
1510.014424	27.064778	65.635214
1509.556181	22.786936	65.640218
1508.894579	19.374017	65.645223
1508.074267	21.182232	65.650228
1507.604851	25.774704	65.655233
1507.272566	22.465570	65.660238
1505.875655	28.927406	65.665242
1505.120226	18.734494	65.670247
1504.773654	21.563385	65.675252
1504.124189	29.589015	65.680257
1503.472879	26.138191	65.685262
1502.521506	23.603925	65.690266
1502.123695	21.525733	65.695271
1501.759712	32.746550	65.700276
1500.709743	18.860012	65.705281
1499.861962	18.914341	65.710286
1499.236743	33.063989	65.715290
1499.076817	20.630277	65.720295
1498.571309	22.230781	65.725300
1497.512889	13.117321	65.730305
1497.183917	16.616754	65.735310
1495.981670	24.345456	65.740314
1494.964244	28.250749	65.745319
1494.429981	33.717676	65.750324
1493.477401	31.866406	65.755329
1493.483750	13.910749	65.760334
1492.832658	27.583547	65.765338
1492.860165	16.050433	65.770343
1491.917559	30.756702	65.775348
1490.956350	25.868100	65.780353
1490.491138	19.211815	65.785358
1489.323912	10.582416	65.790362
1488.584866	16.044032	65.795367
1487.659771	25.982099	65.800372
1487.423842	20.736982	65.805377
1487.149605	12.091833	65.810382
1486.567507	17.470166	65.815386
1485.812557	18.501623	65.820391
1485.065646	17.289439	65.825396
1484.321311	18.387017	65.830401
1483.293882	15.855385	65.835406
1482.348904	25.563230	65.840410
1482.459349	19.931921	65.845415
1482.115691	12.225027	65.850420
1481.285981	13.616862	65.855425
1480.472065	15.290031	65.860430
1479.650218	18.435716	65.865434
1479.379545	8.138982	65.870439
1478.095755	18.633926	65.875444
1477.319949	28.373236	65.880449
1477.098838	13.735277	65.885454
1476.406347	19.503304	65.890458
1476.001453	10.893114	65.895463
1474.882881	11.266441	65.900468
1474.199686	17.859291	65.905473
1474.092429	21.236764	65.910478
1472.992047	13.930813	65.915482
1471.864322	20.140156	65.920487
1471.530583	24.748917	65.925492
1470.884713	14.529151	65.930497
1470.874872	11.796394	65.935502
1469.836162	24.026419	65.940506
1469.004069	23.554731	65.945511
1468.163401	23.051291	65.950516
1468.308765	22.827961	65.955521
1467.479532	22.381049	65.960526
1466.291121	13.255148	65.965530
1465.712189	17.070265	65.970535
1465.167675	18.382091	65.975540
1464.366521	25.681223	65.980545
1463.616624	18.619190	65.985550
1462.905304	21.990160	65.990554
1462.399830	12.568079	65.995559
1461.986465	21.199569	66.000564
1461.016517	16.214604	66.005569
1460.590631	11.556331	66.010574
1459.744628	17.973212	66.015578
1459.346756	14.931546	66.020583
1458.630311	18.035256	66.025588
1457.549487	19.131124	66.030593
1457.387550	17.266183	66.035598
1456.757417	24.255872	66.040602
1456.043829	15.604857	66.045607
1455.115964	13.932598	66.050612
1454.613859	6.894272	66.055617
1454.319330	6.758194	66.060622
1452.777404	6.650047	66.065626
1452.280872	8.555051	66.070631
1451.729666	10.158094	66.075636
1451.086109	13.947214	66.080641
1451.002990	0.634024	66.085646
1450.065450	9.949612	66.090650
1448.984353	11.561174	66.095655
1448.371696	11.362118	66.100660
1447.998986	13.677940	66.105665
1447.430621	6.560263	66.110670
1446.279812	10.832108	66.115674
1446.078370	14.864772	66.120679
1445.445911	15.528277	66.125684
1444.960670	13.393029	66.130689
1443.825978	13.130285	66.135694
1442.732661	17.199037	66.140698
1442.572849	18.345653	66.145703
1442.189371	14.664633	66.150708
1441.574728	12.556259	66.155713
1440.829072	9.803252	66.160718
1439.876224	25.665450	66.165722
1439.414689	13.699147	66.170727
1438.963807	17.855030	66.175732
1437.848924	16.192000	66.180737
1437.304804	11.487868	66.185742
1436.638209	29.190558	66.190746
1436.279914	19.018135	66.195751
1435.453411	16.585474	66.200756
1434.682429	26.819174	66.205761
1434.652074	8.643870	66.210766
1433.433215	17.540566	66.215770
1432.398095	13.584655	66.220775
1431.832345	16.870996	66.225780
1431.760862	15.103642	66.230785
1431.191658	16.804165	66.235790
1429.800779	14.040167	66.240794
1429.514521	13.238900	66.245799
1429.036858	18.316801	66.250804
1427.963532	17.706852	66.255809
1427.159077	11.099772	66.260814
1426.495071	23.090489	66.265818
1426.280616	8.421529	66.270823
1425.923801	12.797422	66.275828
1425.031716	11.810173	66.280833
1424.093680	13.457355	66.285838
1423.201988	19.335898	66.290842
1423.094606	13.035912	66.295847
1422.318109	21.182662	66.300852
1421.167379	24.409019	66.305857
1420.975403	16.635453	66.310862
1420.194234	18.850622	66.315866
1419.793121	13.448850	66.320871
1418.991497	17.512251	66.325876
1418.103707	20.009287	66.330881
1417.660815	19.608219	66.335886
1416.456937	17.817421	66.340890
1415.863120	17.203805	66.345895
1415.341681	14.244864	66.350900
1415.027436	14.332691	66.355905
1414.733000	9.839611	66.360910
1414.103488	18.040268	66.365914
1413.291341	15.766178	66.370919
1412.621381	22.610820	66.375924
1411.263805	23.635578	66.380929
1410.713168	20.280743	66.385934
1409.903275	21.445530	66.390938
1409.487576	19.579925	66.395943
1409.302799	21.392812	66.400948
1408.165301	19.000128	66.405953
1407.280991	12.607591	66.410958
1406.456721	21.318585	66.415962
1406.441590	11.104249	66.420967
1406.118603	12.062342	66.425972
1405.344815	13.145700	66.430977
1404.467144	-0.176810	66.435982
1403.538789	22.365999	66.440986
1403.222468	10.133786	66.445991
1402.042118	15.681332	66.450996
1401.068482	18.162056	66.456001
1400.971980	15.252270	66.461006
1400.588956	22.842915	66.466010
1400.192790	13.132251	66.471015
1399.205515	18.931378	66.476020
1398.334104	22.852918	66.481025
1397.993449	10.295000	66.486030
1397.189144	24.192424	66.491034
1396.499234	14.864329	66.496039
1395.714288	19.290928	66.501044
1395.021740	21.413174	66.506049
1394.760440	7.715158	66.511054
1393.732393	13.326805	66.516058
1393.048373	14.947816	66.521063
1392.521933	12.253018	66.526068
1391.747991	18.026124	66.531073
1390.898840	11.858234	66.536078
1390.179476	21.777815	66.541082
1390.077511	5.451004	66.546087
1389.710145	11.068023	66.551092
1388.617198	13.359563	66.556097
1387.780112	5.685392	66.561102
1387.267973	13.602475	66.566106
1386.527333	9.273359	66.571111
1385.606186	14.872749	66.576116
1384.814986	23.285189	66.581121
1384.813831	17.947580	66.586126
1384.063816	16.679152	66.591130
1383.557615	9.419151	66.596135
1382.538719	12.452684	66.601140
1382.137149	20.312774	66.606145
1381.605126	16.838297	66.611150
1380.339366	13.158759	66.616154
1379.926873	12.152065	66.621159
1379.368372	9.118602	66.626164
1378.629855	12.180108	66.631169
1377.648947	19.105718	66.636174
1376.904452	16.354122	66.641178
1376.793184	11.658473	66.646183
1376.150291	14.345247	66.651188
1375.186696	15.529744	66.656193
1374.349745	5.914385	66.661198
1373.671699	17.852144	66.666202
1373.620310	17.932887	66.671207
1373.158284	20.073688	66.676212
1372.015738	14.616317	66.681217
1371.597522	7.435373	66.686222
1370.678374	26.278886	66.691226
1369.783870	14.611654	66.696231
1369.136147	13.505161	66.701236
1368.405808	12.318764	66.706241
1367.965710	15.365954	66.711246
1367.346777	21.497615	66.716250
1367.135930	17.628324	66.721255
1365.876597	18.673758	66.726260
1365.366803	15.097984	66.731265
1365.181732	10.623797	66.736270
1363.476541	11.978216	66.741274
1363.349488	7.652498	66.746279
1362.830312	19.546083	66.751284
1362.376445	13.719060	66.756289
1361.480865	9.964921	66.761294
1360.667202	19.137849	66.766298
1360.143663	8.513916	66.771303
1359.565491	11.844821	66.776308
1358.824016	15.826139	66.781313
1358.177391	3.212798	66.786318
1357.300907	18.310682	66.791322
1357.150700	11.252712	66.796327
1356.234564	16.994814	66.801332
1355.103980	21.526827	66.806337
1354.433521	14.669822	66.811342
1353.958747	22.580974	66.816346
1353.844927	8.140456	66.821351
1353.094940	12.664006	66.826356
1352.043068	13.919312	66.831361
1351.514608	13.282707	66.836366
1350.925863	15.326963	66.841370
1350.691877	12.454804	66.846375
1349.307000	10.502006	66.851380
1348.828800	14.949239	66.856385
1348.469948	13.412068	66.861390
1347.258277	20.618790	66.866394
1346.739040	15.954879	66.871399
1346.608729	17.210348	66.876404
1345.668051	25.521983	66.881409
1344.753355	18.656497	66.886414
1343.978038	21.335944	66.891418
1344.018392	22.545361	66.896423
1343.333293	26.172382	66.901428
1342.402083	12.112525	66.906433
1341.858477	7.821487	66.911438
1340.977285	17.807797	66.916442
1340.156696	1.076435	66.921447
1339.301318	19.704810	66.926452
1338.316834	13.869104	66.931457
1338.322548	3.705082	66.936462
1337.893689	9.705607	66.941466
1337.217492	14.149625	66.946471
1336.509137	13.387083	66.951476
1335.751050	10.487857	66.956481
1335.347968	9.063372	66.961486
1334.030951	7.434099	66.966490
1333.575471	5.434490	66.971495
1332.539876	10.150098	66.976500
1332.082280	16.943647	66.981505
1332.291492	8.415640	66.986510
1331.135763	23.445963	66.991514
1330.535681	11.181609	66.996519
1329.924785	10.968108	67.001524
1328.882271	24.348340	67.006529
1327.775668	9.620959	67.011534
1327.321034	14.430291	67.016538
1326.968294	9.295232	67.021543
1326.905238	17.781157	67.026548
1326.273196	21.734050	67.031553
1325.443369	17.893779	67.036558
1324.673742	15.214002	67.041562
1324.058262	13.306059	67.046567
1322.960681	19.062824	67.051572
1322.190938	22.159271	67.056577
1322.242507	2.028229	67.061582
1320.676890	17.103210	67.066586
1320.168759	5.062359	67.071591
1319.782981	17.160237	67.076596
1318.938056	8.361428	67.081601
1318.854673	4.878724	67.086606
1317.840498	18.836326	67.091610
1316.938114	10.953371	67.096615
1316.606839	3.090013	67.101620
1316.114710	13.935388	67.106625
1315.523972	2.491128	67.111630
1314.472026	17.307839	67.116634
1313.899677	8.385277	67.121639
1313.411541	7.617695	67.126644
1312.244562	15.135857	67.131649
1311.966508	10.950840	67.136654
1311.187594	9.439455	67.141658
1310.891151	18.243171	67.146663
1309.971572	9.210236	67.151668
1309.006245	19.913230	67.156673
1308.549607	6.157985	67.161678
1307.674092	16.539202	67.166682
1307.484377	5.584684	67.171687
1306.448122	12.834492	67.176692
1305.745295	9.513341	67.181697
1305.505503	0.679840	67.186702
1304.980865	13.115170	67.191706
1304.102114	12.939528	67.196711
1303.449295	11.341869	67.201716
1303.031962	17.395760	67.206721
1302.146088	2.619119	67.211726
1300.952395	17.288061	67.216730
1300.386327	20.006792	67.221735
1300.252783	21.267508	67.226740
1298.794784	20.550040	67.231745
1298.555181	13.927323	67.236750
1297.768163	16.132417	67.241754
1297.378665	12.887608	67.246759
1296.733516	10.872429	67.251764
1296.385157	10.375932	67.256769
1295.589447	13.374014	67.261774
1294.867693	12.785498	67.266778
1294.408532	17.179251	67.271783
1293.159626	17.062461	67.276788
1292.610122	20.142825	67.281793
1292.198479	22.583125	67.286798
1291.372860	17.017063	67.291802
1290.625509	14.959788	67.296807
1289.872776	8.669382	67.301812
1289.380705	9.033069	67.306817
1289.170214	1.708740	67.311822
1288.077351	20.567260	67.316826
1287.422232	23.809492	67.321831
1287.002891	16.245555	67.326836
1286.296907	10.422365	67.331841
1285.590272	4.969853	67.336846
1284.690044	14.591782	67.341850
1284.109850	6.589814	67.346855
1283.914835	9.293707	67.351860
1282.400674	15.227099	67.356865
1282.387926	10.107378	67.361870
1281.789103	17.331804	67.366874
1281.193828	11.746472	67.371879
1279.886235	7.777181	67.376884
1279.190561	13.034836	67.381889
1278.998068	15.645292	67.386894
1278.339487	11.184898	67.391898
1277.203946	19.232648	67.396903
1276.849918	7.570998	67.401908
1276.141430	6.239233	67.406913
1276.230704	5.179589	67.411918
1274.643876	11.660683	67.416922
1273.942644	4.930025	67.421927
1273.634373	10.085087	67.426932
1273.229926	4.806878	67.431937
1272.416824	6.473671	67.436942
1271.513605	8.362943	67.441946
1271.222445	7.430015	67.446951
1270.477556	11.722546	67.451956
1269.570703	12.940636	67.456961
1268.974809	10.852980	67.461966
1268.037400	14.389247	67.466970
1267.712638	5.512491	67.471975
1266.524428	5.505908	67.476980
1265.726249	6.929064	67.481985
1265.351064	7.539092	67.486990
1264.733747	15.632180	67.491994
1264.600188	5.813574	67.496999
1264.118628	8.359606	67.502004
1263.327958	17.014827	67.507009
1262.438883	7.477186	67.512014
1262.044359	8.281095	67.517018
1261.312277	7.495540	67.522023
1260.552598	14.450662	67.527028
1259.997273	15.393675	67.532033
1259.060102	9.985709	67.537038
1257.914805	13.228613	67.542042
1257.962088	13.194325	67.547047
1257.575310	14.053772	67.552052
1256.402234	18.510579	67.557057
1255.511403	6.126910	67.562062
1254.791379	11.287519	67.567066
1254.517485	12.129018	67.572071
1253.858931	12.142303	67.577076
1253.049024	6.662068	67.582081
1252.809191	9.805160	67.587086
1251.872694	16.461980	67.592090
1251.270593	12.123497	67.597095
1250.092472	11.293750	67.602100
1249.541586	15.487635	67.607105
1249.487488	12.307774	67.612110
1248.569532	21.883651	67.617114
1247.665511	17.170562	67.622119
1247.026183	11.026137	67.627124
1246.422981	9.007456	67.632129
1246.263456	6.963961	67.637134
1244.729105	14.374986	67.642138
1244.403724	5.902021	67.647143
1244.032899	5.571525	67.652148
1243.333913	11.162439	67.657153
1243.023151	18.336338	67.662158
1241.622694	22.420889	67.667162
1241.355547	9.360910	67.672167
1240.912557	16.781331	67.677172
1239.667550	10.252257	67.682177
1239.573219	14.758313	67.687182
1238.855756	17.404937	67.692186
1237.508214	20.055554	67.697191
1236.715171	10.234581	67.702196
1236.162870	10.458050	67.707201
1236.123545	10.301918	67.712206
1235.579679	14.475766	67.717210
1235.134464	1.753182	67.722215
1233.949690	13.691106	67.727220
1233.425070	10.399988	67.732225
1233.140335	7.906485	67.737230
1231.666465	18.062751	67.742234
1231.186226	15.682334	67.747239
1230.621600	16.029185	67.752244
1229.931642	16.717654	67.757249
1229.232221	8.207974	67.762254
1228.251149	15.742338	67.767258
1227.845978	16.100104	67.772263
1227.660880	16.287264	67.777268
1227.061717	15.091088	67.782273
1226.121055	7.261569	67.787278
1225.491434	20.013216	67.792282
1224.705858	14.469198	67.797287
1223.989682	2.273811	67.802292
1222.930134	19.124381	67.807297
1222.794485	6.962835	67.812302
1222.276128	15.926413	67.817306
1221.815281	7.132804	67.822311
1220.769689	8.439201	67.827316
1220.126195	12.513778	67.832321
1219.780686	12.329066	67.837326
1218.389175	18.082145	67.842330
1217.834898	13.357609	67.847335
1217.666985	11.066299	67.852340
1217.037781	10.854160	67.857345
1216.039523	4.296905	67.862350
1215.057227	13.826248	67.867354
1214.716172	10.628943	67.872359
1214.461834	1.160703	67.877364
1213.711444	22.304907	67.882369
1213.072361	12.932531	67.887374
1212.172827	15.401538	67.892378
1211.276298	1.558588	67.897383
1210.469230	3.306438	67.902388
1209.663685	9.568718	67.907393
1209.464724	9.739160	67.912398
1209.019585	14.375115	67.917402
1208.622309	6.572734	67.922407
1207.543686	18.437023	67.927412
1206.604245	14.533805	67.932417
1206.680164	6.389683	67.937422
1205.964843	11.623669	67.942426
1204.685099	12.374392	67.947431
1204.223085	22.781344	67.952436
1203.474671	18.097143	67.957441
1203.292671	11.162518	67.962446
1201.923453	12.499885	67.967450
1201.548197	13.480506	67.972455
1201.486198	16.109638	67.977460
1200.200518	9.194405	67.982465
1199.380446	9.687537	67.987470
1198.748625	17.284641	67.992474
1198.459375	2.542484	67.997479
1197.912097	5.917389	68.002484
1196.559362	21.378032	68.007489
1196.464648	1.115742	68.012494
1195.753307	7.831384	68.017498
1195.010698	7.427556	68.022503
1194.292341	8.681927	68.027508
1193.444385	12.461028	68.032513
1193.269968	12.017307	68.037518
1192.470361	6.336768	68.042522
1191.598791	11.229763	68.047527
1191.165511	13.466942	68.052532
1190.480878	16.914154	68.057537
1189.971066	0.727941	68.062542
1188.340835	18.735255	68.067546
1187.957462	6.061193	68.072551
1187.943856	8.450824	68.077556
1187.360336	10.445398	68.082561
1186.914152	-1.807097	68.087566
1185.471199	14.889989	68.092570
1185.199224	11.173941	68.097575
1184.852113	2.401681	68.102580
1183.531175	7.034989	68.107585
1182.948089	10.877624	68.112590
1182.334351	7.909763	68.117594
1181.925818	9.231558	68.122599
1180.996488	-3.532285	68.127604
1180.282628	2.784802	68.132609
1179.608700	-1.236315	68.137614
1179.317097	10.562741	68.142618
1178.480699	11.211434	68.147623
1177.564357	7.288787	68.152628
1176.735412	9.664581	68.157633
1176.746720	-1.542641	68.162638
1176.155712	10.010724	68.167642
1175.144456	-4.886250	68.172647
1174.878448	-2.749786	68.177652
1174.323782	20.629298	68.182657
1173.283789	4.090599	68.187662
1172.390547	-1.341657	68.192666
1172.139381	-2.489084	68.197671
1171.547934	6.664307	68.202676
1169.994371	9.767176	68.207681
1169.597556	5.774528	68.212686
1169.048972	11.300540	68.217690
1168.874439	14.794364	68.222695
1168.093913	1.472289	68.227700
1166.839244	5.011734	68.232705
1166.806674	1.464192	68.237710
1165.977945	6.087038	68.242714
1165.465724	5.455775	68.247719
1164.414008	9.257826	68.252724
1163.452407	13.993266	68.257729
1163.580735	6.280768	68.262734
1162.773001	10.701587	68.267738
1161.900242	6.535481	68.272743
1161.491619	8.084366	68.277748
1160.627399	21.951931	68.282753
1160.184836	6.204446	68.287758
1159.116067	14.855031	68.292762
1158.534082	22.758022	68.297767
1158.273473	16.143399	68.302772
1157.414289	14.980709	68.307777
1156.811049	4.328521	68.312782
1155.634277	10.110552	68.317786
1155.342444	13.665608	68.322791
1155.137583	6.796127	68.327796
1153.983533	7.273003	68.332801
1153.399344	8.021938	68.337806
1152.706242	12.821909	68.342810
1152.152013	19.574078	68.347815
1151.366169	14.454316	68.352820
1150.457020	6.719165	68.357825
1150.256668	4.792555	68.362830
1149.436772	15.376266	68.367834
1148.719697	16.286681	68.372839
1147.938502	23.965899	68.377844
1147.500145	13.052526	68.382849
1147.495998	6.069127	68.387854
1145.931591	14.251357	68.392858
1145.570192	4.374393	68.397863
1144.942554	4.767553	68.402868
1143.662969	9.851604	68.407873
1142.837375	14.268962	68.412878
1142.288353	16.906167	68.417882
1142.028051	11.731211	68.422887
1141.637581	7.534139	68.427892
1141.558219	8.030906	68.432897
1140.731880	12.978222	68.437902
1139.947516	8.812257	68.442906
1138.967294	9.207879	68.447911
1137.805261	23.223736	68.452916
1137.186681	6.231692	68.457921
1137.426140	13.346469	68.462926
1136.171197	11.533970	68.467930
1135.445504	7.035411	68.472935
1135.092522	-4.408746	68.477940
1134.382525	10.033506	68.482945
1133.984918	21.634970	68.487950
1132.756176	21.647511	68.492954
1132.498209	2.439342	68.497959
1131.334338	14.988967	68.502964
1130.372628	11.571855	68.507969
1129.980024	9.420365	68.512974
1129.270392	5.398632	68.517978
1129.349300	3.189496	68.522983
1128.639932	6.200699	68.527988
1127.407468	8.829913	68.532993
1126.971735	14.470444	68.537998
1126.326770	7.199471	68.543002
1126.119357	10.454105	68.548007
1125.036790	10.698859	68.553012
1124.072386	8.955271	68.558017
1124.036980	3.530093	68.563022
1123.364325	15.331412	68.568026
1122.429811	5.457299	68.573031
1121.493657	9.837055	68.578036
1121.017724	15.135486	68.583041
1120.136889	6.277822	68.588046
1119.328995	15.039887	68.593050
1118.728360	3.792808	68.598055
1118.564770	-2.387814	68.603060
1117.868392	11.975007	68.608065
1116.959636	6.456932	68.613070
1116.309690	9.280497	68.618074
1115.887631	-2.649394	68.623079
1115.634518	1.167576	68.628084
1114.348158	17.549636	68.633089
1114.116272	5.920641	68.638094
1113.103270	10.460852	68.643098
1112.233925	2.221088	68.648103
1111.343754	13.164478	68.653108
1110.787714	15.484270	68.658113
1110.664793	8.354189	68.663118
1109.986647	5.054406	68.668122
1109.193315	2.984004	68.673127
1108.446169	7.688503	68.678132
1107.761790	13.849539	68.683137
1107.535436	-3.050330	68.688142
1106.289309	9.427230	68.693146
1105.598833	8.751794	68.698151
1105.523822	5.163698	68.703156
1104.552385	23.567725	68.708161
1103.575570	1.236523	68.713166
1102.668789	17.627596	68.718170
1102.381501	7.658430	68.723175
1102.094651	6.926681	68.728180
1101.650132	13.623558	68.733185
1100.633929	13.868805	68.738190
1100.047410	20.350160	68.743194
1099.307610	9.667672	68.748199
1098.032132	2.984261	68.753204
1097.159527	14.681773	68.758209
1096.949649	4.410148	68.763214
1096.821231	10.578946	68.768218
1096.484097	3.124985	68.773223
1095.541333	14.694890	68.778228
1094.548437	22.396753	68.783233
1094.203165	-4.279907	68.788238
1093.505240	12.610933	68.793242
1092.610903	9.627807	68.798247
1091.935688	0.166615	68.803252
1091.100898	8.467776	68.808257
1090.584459	10.319240	68.813262
1089.669835	13.348910	68.818266
1089.530702	10.390736	68.823271
1089.379978	2.716321	68.828276
1087.990082	13.587822	68.833281
1087.407489	4.919269	68.838286
1086.751015	12.895613	68.843290
1086.165947	10.460941	68.848295
1085.083139	3.504048	68.853300
1084.224047	4.752449	68.858305
1084.067222	-1.094942	68.863310
1083.736887	2.857311	68.868314
1082.893614	-2.522934	68.873319
1081.769291	-0.374510	68.878324
1081.239774	0.923967	68.883329
1081.175313	-6.869815	68.888334
1079.703007	8.326034	68.893338
1079.188601	7.162145	68.898343
1078.765773	7.711971	68.903348
1078.432960	1.205044	68.908353
1077.779217	5.727542	68.913358
1076.624654	12.297677	68.918362
1075.739859	5.544248	68.923367
1075.495515	9.798206	68.928372
1074.707482	10.521238	68.933377
1074.044354	7.014079	68.938382
1073.328448	6.132970	68.943386
1072.837758	6.816590	68.948391
1072.921039	7.833095	68.953396
1071.704765	17.010204	68.958401
1070.943423	10.738592	68.963406
1069.580020	16.400542	68.968410
1068.772277	19.195606	68.973415
1068.740317	3.004385	68.978420
1068.004485	6.368307	68.983425
1068.024889	17.263056	68.988430
1067.337854	10.427710	68.993434
1066.383220	0.684557	68.998439
1065.771446	9.763928	69.003444
1064.958715	-4.598456	69.008449
1064.178520	5.996297	69.013454
1063.090795	9.228545	69.018458
1062.766312	1.296357	69.023463
1062.373360	6.154252	69.028468
1061.371785	1.384225	69.033473
1060.811607	9.042488	69.038478
1059.984138	6.536000	69.043482
1059.726215	9.133220	69.048487
1059.490309	6.214097	69.053492
1058.458826	17.094828	69.058497
1057.656050	3.181850	69.063502
1057.235974	17.604806	69.068506
1056.215903	15.549989	69.073511
1055.403394	16.404650	69.078516
1054.376714	16.340932	69.083521
1054.367700	3.749282	69.088526
1054.120277	2.208625	69.093530
1053.174875	0.889382	69.098535
1052.308013	6.790882	69.103540
1051.638379	14.543830	69.108545
1051.127697	1.710297	69.113550
1050.067715	7.609404	69.118554
1049.681282	6.357357	69.123559
1048.938910	12.360478	69.128564
1048.823627	11.686595	69.133569
1047.871336	0.446600	69.138574
1047.408480	3.637796	69.143578
1046.691083	-2.196106	69.148583
1045.579970	-2.910263	69.153588
1044.838761	10.644441	69.158593
1044.375616	2.535625	69.163598
1044.069139	4.508233	69.168602
1042.834159	5.296067	69.173607
1042.198875	1.284613	69.178612
1041.610278	19.951008	69.183617
1041.324758	8.119255	69.188622
1040.131982	1.913137	69.193626
1039.218855	-1.145822	69.198631
1039.304358	-2.906590	69.203636
1038.609358	9.969004	69.208641
1037.965156	5.889585	69.213646
1036.728884	11.193868	69.218650
1036.357305	4.812960	69.223655
1036.040268	1.780595	69.228660
1035.498594	11.250929	69.233665
1034.805327	-1.976157	69.238670
1033.490018	4.974365	69.243674
1033.555119	15.560809	69.248679
1032.569818	10.578475	69.253684
1031.595854	2.658155	69.258689
1031.278311	6.594187	69.263694
1030.658899	5.213631	69.268698
1030.061050	-0.379096	69.273703
1029.265385	10.448355	69.278708
1028.628118	8.299536	69.283713
1028.212582	6.079176	69.288718
1026.944865	0.397480	69.293722
1026.521433	-3.460020	69.298727
1026.065854	5.517238	69.303732
1025.296247	11.535735	69.308737
1024.823452	2.067595	69.313742
1023.439290	15.137986	69.318746
1023.092186	2.656895	69.323751
1022.732222	-3.946620	69.328756
1021.862958	21.967700	69.333761
1021.367469	4.841012	69.338766
1020.494810	2.512033	69.343770
1020.040191	0.785154	69.348775
1019.450647	8.657821	69.353780
1018.298493	13.560813	69.358785
1018.160910	7.746634	69.363790
1017.352610	-8.565475	69.368794
1016.771813	5.244395	69.373799
1015.782422	6.026287	69.378804
1015.049756	16.774339	69.383809
1014.832789	8.162754	69.388814
1014.468801	0.886544	69.393818
1013.541525	8.393487	69.398823
1012.927146	10.643734	69.403828
1012.270551	1.403529	69.408833
1011.097503	4.039112	69.413838
1010.306460	6.173966	69.418842
1009.840031	-2.345886	69.423847
1009.705941	0.786703	69.428852
1008.612809	4.827204	69.433857
1007.977924	6.637606	69.438862
1007.173670	2.222550	69.443866
1007.210114	-0.072867	69.448871
1006.506224	4.872348	69.453876
1005.497283	8.792228	69.458881
1005.062176	-1.393081	69.463886
1004.103632	12.148900	69.468890
1003.210724	-0.150735	69.473895
1002.639541	-11.329909	69.478900
1002.227431	6.735979	69.483905
1001.694252	4.772451	69.488910
1000.614436	7.907275	69.493914
1000.085530	-1.756925	69.498919
999.303097	1.034129	69.503924
999.245219	13.013611	69.508929
998.471437	-2.860879	69.513934
997.126081	14.894619	69.518938
996.911895	2.731421	69.523943
996.545788	2.449095	69.528948
995.288910	4.292227	69.533953
994.886177	-2.331285	69.538958
993.981404	9.623667	69.543962
993.737961	10.258503	69.548967
992.604665	-0.716131	69.553972
991.921510	12.502928	69.558977
991.581467	-3.749637	69.563982
991.389525	9.145271	69.568986
990.414879	9.506948	69.573991
989.464623	5.700157	69.578996
988.772063	7.839849	69.584001
988.958594	4.462454	69.589006
987.506834	4.863773	69.594010
986.772614	4.591132	69.599015
986.448511	6.255901	69.604020
985.764512	0.393051	69.609025
985.080431	2.081979	69.614030
983.978108	9.216250	69.619034
983.793843	8.021931	69.624039
983.260931	3.909053	69.629044
982.213760	8.506782	69.634049
981.759481	-8.380435	69.639054
980.932406	5.320394	69.644058
980.163195	6.795794	69.649063
979.359834	0.040491	69.654068
978.664237	8.713757	69.659073
978.502265	3.433302	69.664078
977.941641	6.094458	69.669082
977.525699	2.869688	69.674087
976.689152	-6.756592	69.679092
975.745456	8.085546	69.684097
975.031432	-5.377898	69.689102
974.038065	7.450561	69.694106
973.376736	-2.985740	69.699111
973.009314	6.858982	69.704116
972.509320	-0.073892	69.709121
972.176873	-1.791815	69.714126
971.087931	5.630479	69.719130
970.696652	8.349844	69.724135
969.663811	3.747253	69.729140
968.646180	4.552578	69.734145
968.471951	4.260227	69.739150
967.578532	2.983207	69.744154
967.526783	-7.908033	69.749159
966.463200	5.046711	69.754164
965.761845	4.612734	69.759169
965.374608	8.031600	69.764174
964.989035	3.985167	69.769178
963.858332	0.576092	69.774183
963.198756	4.252748	69.779188
962.547812	2.274853	69.784193
961.520057	-0.048349	69.789198
960.822091	1.223339	69.794202
960.313347	8.234788	69.799207
960.164057	-0.770736	69.804212
959.206068	11.169039	69.809217
958.451912	3.002474	69.814222
957.886988	2.411178	69.819226
957.731634	2.598355	69.824231
956.688105	1.974406	69.829236
955.374242	7.251645	69.834241
955.340653	1.619619	69.839246
955.056895	15.221397	69.844250
953.940395	10.200051	69.849255
953.106704	-2.296630	69.854260
952.361416	8.300476	69.859265
952.459125	8.981955	69.864270
950.990668	9.923674	69.869274
950.451335	-3.428791	69.874279
949.782340	-7.638271	69.879284
949.252447	-0.667612	69.884289
949.303396	0.383993	69.889294
948.038562	9.994633	69.894298
947.535229	11.970190	69.899303
946.675505	4.977870	69.904308
945.573988	5.796552	69.909313
945.163283	-5.212606	69.914318
944.482515	1.036188	69.919322
944.005075	3.982148	69.924327
943.564055	-0.651524	69.929332
942.188309	3.998501	69.934337
942.335180	-0.582064	69.939342
941.440586	2.655769	69.944346
941.025606	-1.857471	69.949351
940.186249	1.770528	69.954356
939.303173	17.249564	69.959361
939.077809	7.328927	69.964366
937.525917	8.186162	69.969370
937.002461	5.475230	69.974375
936.951076	5.797246	69.979380
936.181221	6.151588	69.984385
936.037691	-9.066240	69.989390
934.491913	2.359959	69.994394
934.311323	2.499114	69.999399
933.591627	-2.656317	70.004404
932.406840	12.608960	70.009409
931.885530	3.585367	70.014414
931.012217	-1.209740	70.019418
930.646338	7.702793	70.024423
930.488045	3.736891	70.029428
929.459841	5.551552	70.034433
928.560054	-5.466506	70.039438
928.045942	9.241055	70.044442
927.605303	1.018308	70.049447
927.485111	7.937971	70.054452
926.272341	9.433508	70.059457
925.884119	4.007720	70.064462
924.315194	0.613205	70.069466
923.558251	5.617341	70.074471
923.253245	11.951426	70.079476
922.730644	8.647447	70.084481
922.593637	0.256541	70.089486
921.970800	10.378445	70.094490
921.449951	13.079014	70.099495
920.786685	4.734002	70.104500
919.537151	5.778092	70.109505
918.982319	-4.296678	70.114510
918.212108	4.167703	70.119514
917.667077	-0.969788	70.124519
916.639620	4.805922	70.129524
915.955199	0.117952	70.134529
916.114642	-0.686370	70.139534
915.009442	12.886854	70.144538
914.069173	-1.545049	70.149543
913.712399	-8.830264	70.154548
912.716495	-6.319020	70.159553
912.659626	2.944869	70.164558
911.350655	5.160594	70.169562
910.736621	2.640695	70.174567
910.562050	-0.729700	70.179572
909.864854	7.803488	70.184577
909.237819	-5.910305	70.189582
908.370497	-1.639205	70.194586
907.685813	13.910761	70.199591
907.351604	-6.526211	70.204596
905.840141	4.694277	70.209601
905.656856	-2.768353	70.214606
904.815466	0.561946	70.219610
904.539934	0.000302	70.224615
903.624060	1.248336	70.229620
902.858353	6.108798	70.234625
902.672604	-4.411041	70.239630
902.159213	3.170412	70.244634
901.155179	0.824538	70.249639
900.368492	-4.528371	70.254644
899.705898	1.712811	70.259649
899.219712	-7.188626	70.264654
898.188715	5.396689	70.269658
897.452571	3.825017	70.274663
897.229428	-3.788957	70.279668
896.688950	1.606498	70.284673
896.047624	-0.248334	70.289678
895.303413	11.657437	70.294682
894.513242	11.016848	70.299687
893.614933	-0.034547	70.304692
892.357803	-0.078871	70.309697
892.384889	-5.542356	70.314702
891.178201	-4.754221	70.319706
891.181096	3.571364	70.324711
890.859812	7.489081	70.329716
890.261335	-0.542964	70.334721
889.497978	-0.981244	70.339726
888.630437	-6.075285	70.344730
888.080325	9.642490	70.349735
887.019716	-5.076162	70.354740
886.193163	1.284152	70.359745
886.148077	-7.908244	70.364750
885.415042	1.357597	70.369754
884.545369	0.769086	70.374759
883.921116	9.590281	70.379764
883.366161	7.958241	70.384769
882.661482	-0.383317	70.389774
881.781843	4.886351	70.394778
881.425848	-2.832631	70.399783
880.945107	1.742796	70.404788
879.717359	12.348892	70.409793
879.337421	-3.570871	70.414798
878.910267	10.033220	70.419802
878.169054	9.504689	70.424807
877.292485	-2.808519	70.429812
876.329837	7.799538	70.434817
876.278505	-2.427887	70.439822
874.945335	3.002266	70.444826
874.276227	2.000231	70.449831
873.952284	-9.147286	70.454836
873.065021	8.377651	70.459841
873.028763	6.823908	70.464846
872.526800	6.526953	70.469850
871.517440	0.843651	70.474855
871.126395	6.112832	70.479860
869.743932	8.456964	70.484865
869.116443	9.927187	70.489870
868.053375	10.282484	70.494874
868.183955	-1.243293	70.499879
867.540175	9.474864	70.504884
867.116978	1.692464	70.509889
866.183597	2.662610	70.514894
865.605128	0.934973	70.519898
864.880939	3.142805	70.524903
864.229951	6.270933	70.529908
863.168117	2.961329	70.534913
863.001495	-0.620052	70.539918
861.958631	-6.091442	70.544922
861.057267	-4.153445	70.549927
860.473030	-8.229735	70.554932
859.925804	3.285152	70.559937
859.849921	-6.181451	70.564942
858.792027	-1.816930	70.569946
857.746812	5.588982	70.574951
857.176353	2.899743	70.579956
856.927482	3.480263	70.584961
856.347448	4.182873	70.589966
855.396072	2.878851	70.594970
854.780220	2.260992	70.599975
854.568125	3.963141	70.604980
853.534246	12.775422	70.609985
852.862975	-1.467456	70.614990
852.058887	2.673753	70.619994
851.621232	8.841301	70.624999
851.205270	5.616559	70.630004
850.086472	4.757062	70.635009
849.778829	-1.963549	70.640014
849.115386	-0.858170	70.645018
848.266808	-0.932803	70.650023
847.544062	-1.390149	70.655028
846.934131	8.843247	70.660033
846.694833	-3.815791	70.665038
845.326948	4.616001	70.670042
844.768980	13.965954	70.675047
844.342284	-2.613384	70.680052
843.686197	3.447007	70.685057
842.977485	0.295669	70.690062
842.217029	7.601074	70.695066
841.572069	-0.710551	70.700071
841.216294	-3.657873	70.705076
840.048112	2.484023	70.710081
839.656516	-9.190440	70.715086
839.096665	-0.657027	70.720090
838.564212	3.428338	70.725095
837.902976	-3.669638	70.730100
836.972475	6.832391	70.735105
836.483505	-4.301470	70.740110
835.552778	-0.856011	70.745114
834.415540	12.831141	70.750119
834.404786	-8.817879	70.755124
833.854203	-3.177966	70.760129
833.536634	-2.214362	70.765134
832.259970	11.504442	70.770138
831.784685	1.897988	70.775143
831.432485	-2.721410	70.780148
830.233301	7.284088	70.785153
829.697131	4.701357	70.790158
828.888264	7.643317	70.795162
828.358320	0.576483	70.800167
828.046152	3.258044	70.805172
826.832376	4.534598	70.810177
826.497002	-2.088557	70.815182
825.898461	5.853375	70.820186
825.340048	7.350460	70.825191
824.412245	2.776948	70.830196
823.589097	7.640264	70.835201
823.302513	-8.660173	70.840206
822.369763	7.870684	70.845210
821.654419	3.820000	70.850215
821.343013	-4.511592	70.855220
820.496032	5.609731	70.860225
820.710258	-2.400263	70.865230
819.152385	6.481236	70.870234
818.483644	5.958534	70.875239
817.746968	2.144627	70.880244
816.690316	1.418751	70.885249
816.440976	-4.588914	70.890254
815.602865	0.786121	70.895258
815.412907	2.390134	70.900263
815.210330	-6.531190	70.905268
813.722525	-3.670388	70.910273
813.222412	8.384191	70.915278
812.603413	4.179408	70.920282
811.970244	6.626646	70.925287
810.714722	-5.205178	70.930292
810.243320	2.888400	70.935297
809.759858	-2.856504	70.940302
809.419636	7.813342	70.945306
808.964305	-2.261462	70.950311
808.241400	1.546728	70.955316
807.289319	1.822884	70.960321
806.794810	-6.928973	70.965326
805.550468	7.599946	70.970330
805.232294	5.875044	70.975335
804.696279	4.443428	70.980340
804.316875	4.097017	70.985345
803.169160	-7.941188	70.990350
802.532640	12.002230	70.995354
802.294122	-1.716597	71.000359
801.697060	0.439478	71.005364
800.511398	2.703436	71.010369
799.958508	-1.538672	71.015374
799.587858	5.868692	71.020378
798.827218	1.468847	71.025383
798.068055	-5.160958	71.030388
797.392723	-4.184555	71.035393
796.785577	-4.007453	71.040398
795.712765	0.239622	71.045402
795.165970	-2.092259	71.050407
795.035763	-0.822596	71.055412
794.503064	2.663596	71.060417
793.262747	-10.965139	71.065422
792.795556	-0.516353	71.070426
792.345576	-0.086734	71.075431
791.798916	-6.307255	71.080436
790.543758	-4.820678	71.085441
789.734830	-1.432437	71.090446
789.585903	1.040222	71.095450
788.983161	-1.697475	71.100455
788.133492	-5.722032	71.105460
787.286360	-1.233345	71.110465
787.051841	2.495532	71.115470
786.265059	5.703638	71.120474
785.268550	9.314124	71.125479
784.448205	0.410716	71.130484
784.123165	9.163797	71.135489
784.083388	3.100699	71.140494
782.944829	0.915056	71.145498
781.800427	-7.220851	71.150503
781.492302	0.611780	71.155508
780.795194	3.835574	71.160513
780.777689	4.779804	71.165518
779.751390	7.896734	71.170522
778.823436	-0.912273	71.175527
777.989379	-3.797641	71.180532
777.033692	7.203557	71.185537
776.774827	-2.781091	71.190542
776.407006	2.903855	71.195546
776.134156	-3.178906	71.200551
775.151213	4.687035	71.205556
774.063955	12.558548	71.210561
773.976262	-7.337320	71.215566
772.796240	0.332920	71.220570
771.791831	4.949147	71.225575
771.698485	-2.674430	71.230580
770.986265	-2.406481	71.235585
770.608313	-7.278800	71.240590
769.392900	4.667303	71.245594
768.760039	3.249535	71.250599
768.392978	0.408096	71.255604
767.740208	3.232188	71.260609
766.867444	-6.344081	71.265614
766.211816	0.823230	71.270618
765.772404	1.426206	71.275623
765.348070	1.410217	71.280628
764.298499	-3.249536	71.285633
763.425706	2.067959	71.290638
762.824949	13.786920	71.295642
762.395592	10.283640	71.300647
761.899611	-0.924775	71.305652
760.809644	-4.838532	71.310657
760.494857	-2.891381	71.315662
759.756171	10.401197	71.320666
759.488100	0.834316	71.325671
758.238044	-4.954112	71.330676
757.650118	15.754254	71.335681
757.285966	2.377121	71.340686
756.602018	-5.507234	71.345690
755.389229	2.653912	71.350695
755.002690	2.217185	71.355700
754.213148	2.481679	71.360705
754.167942	-1.514820	71.365710
753.153887	12.988500	71.370714
752.596272	0.149928	71.375719
752.520312	2.010177	71.380724
751.078235	-1.639373	71.385729
750.386638	-4.058573	71.390734
749.997811	2.697275	71.395738
748.980986	7.862671	71.400743
748.374397	5.056213	71.405748
747.446606	11.144111	71.410753
747.369791	-4.215182	71.415758
746.800626	1.717853	71.420762
745.630727	9.224075	71.425767
745.205792	4.042281	71.430772
744.261476	6.807141	71.435777
744.269089	3.032459	71.440782
743.373740	13.092121	71.445786
742.491010	5.277256	71.450791
742.188420	-1.316410	71.455796
741.302949	2.440409	71.460801
740.555211	-7.428554	71.465806
739.790683	-0.493051	71.470810
739.214772	0.894877	71.475815
739.107185	-11.039227	71.480820
737.815288	-9.933115	71.485825
737.388088	-6.706552	71.490830
736.649919	-2.648343	71.495834
735.529214	0.817933	71.500839
734.907527	6.166422	71.505844
734.389011	3.333331	71.510849
733.996342	-12.414043	71.515854
733.611782	2.760155	71.520858
732.928799	-2.699085	71.525863
732.247977	-2.786194	71.530868
731.364964	4.751626	71.535873
730.766001	-4.551262	71.540878
729.734486	-6.534732	71.545882
729.004924	3.063311	71.550887
728.793877	8.411078	71.555892
728.264239	-2.222708	71.560897
727.544526	-5.067916	71.565902
726.378067	8.587647	71.570906
726.202253	4.996704	71.575911
725.835668	-9.499616	71.580916
724.641656	8.892588	71.585921
724.010716	-0.053562	71.590926
723.443911	4.920351	71.595930
722.558733	9.653228	71.600935
722.043024	5.108764	71.605940
721.506312	0.296419	71.610945
721.341231	-2.266520	71.615950
720.147937	7.692351	71.620954
719.274758	-3.254153	71.625959
719.123282	4.432122	71.630964
717.910365	3.420519	71.635969
717.272627	10.993411	71.640974
716.571594	4.619295	71.645978
716.038634	2.796144	71.650983
715.874601	1.123983	71.655988
714.807599	13.585781	71.660993
714.474831	8.378280	71.665998
713.650389	11.277025	71.671002
712.818546	8.116946	71.676007
712.101635	7.322832	71.681012
711.729530	7.421534	71.686017
711.511636	7.139307	71.691022
709.988934	16.469415	71.696026
709.174100	8.553870	71.701031
708.991252	10.718132	71.706036
708.265405	14.854812	71.711041
707.154569	12.365180	71.716046
706.361413	14.826878	71.721050
705.913085	5.785426	71.726055
705.748219	9.096381	71.731060
705.180355	5.919507	71.736065
704.549269	4.738007	71.741070
703.830164	13.504950	71.746074
703.093191	4.922602	71.751079
702.111986	7.253397	71.756084
701.288895	11.921204	71.761089
701.139557	5.290528	71.766094
700.325488	6.170779	71.771098
699.747296	7.568540	71.776103
698.821792	6.993715	71.781108
698.147472	12.126674	71.786113
697.955766	10.455765	71.791118
697.213008	11.920729	71.796122
695.949164	11.857073	71.801127
695.837092	-5.567056	71.806132
694.836616	-6.044790	71.811137
694.560115	3.533161	71.816142
693.614761	10.874348	71.821146
692.989961	2.718829	71.826151
692.710835	1.468679	71.831156
691.342567	14.068335	71.836161
690.460178	7.488145	71.841166
690.069978	15.349625	71.846170
689.772643	10.847665	71.851175
689.519956	6.570401	71.856180
688.457806	18.164148	71.861185
688.178667	5.842630	71.866190
687.685078	6.236635	71.871194
686.345714	-2.669242	71.876199
685.698081	-0.856737	71.881204
684.839126	8.941684	71.886209
684.435924	9.379644	71.891214
683.587205	3.681889	71.896218
682.931676	6.370827	71.901223
682.395857	1.678194	71.906228
681.639670	-1.060272	71.911233
681.285937	-1.524287	71.916238
680.441535	6.012131	71.921242
679.683826	3.128833	71.926247
679.477858	-4.038424	71.931252
678.779680	5.305483	71.936257
677.449884	3.014727	71.941262
676.853716	-2.753196	71.946266
676.635540	8.583167	71.951271
676.439199	0.411472	71.956276
674.901144	10.157184	71.961281
674.359579	-0.588223	71.966286
673.945762	-0.061843	71.971290
673.477572	13.752208	71.976295
672.615436	-4.826617	71.981300
671.462905	8.183375	71.986305
671.481692	-10.057911	71.991310
670.548493	7.490141	71.996314
669.802423	11.734124	72.001319
669.560383	9.891468	72.006324
669.038374	-3.307541	72.011329
667.930131	-5.534223	72.016334
667.072038	1.897148	72.021338
666.782749	6.257625	72.026343
666.479139	1.471254	72.031348
665.267218	13.241810	72.036353
664.513432	-5.325878	72.041358
663.942393	1.506297	72.046362
662.813291	3.803887	72.051367
662.194278	-5.497362	72.056372
661.164806	17.364388	72.061377
661.338200	6.691210	72.066382
660.878840	3.490763	72.071386
660.469821	-3.190014	72.076391
659.885570	2.712323	72.081396
658.955090	8.859020	72.086401
658.049826	-2.217959	72.091406
657.340678	7.876723	72.096410
656.454903	6.767329	72.101415
656.299337	-0.218725	72.106420
655.242581	2.362227	72.111425
654.154360	-0.417973	72.116430
653.935536	9.486676	72.121434
653.093992	12.949536	72.126439
653.319231	-9.670536	72.131444
652.380575	5.230785	72.136449
651.462677	-3.907755	72.141454
651.093842	7.528288	72.146458
650.218931	4.824505	72.151463
649.378537	-3.287204	72.156468
648.490654	1.343626	72.161473
648.396806	2.019324	72.166478
647.598948	-1.439442	72.171482
646.488863	-6.775450	72.176487
646.078974	-4.668070	72.181492
645.591899	7.064333	72.186497
645.169001	0.511919	72.191502
643.804728	0.383861	72.196506
643.019520	1.239033	72.201511
642.678743	-3.897791	72.206516
642.306314	-4.251594	72.211521
641.686030	-6.548081	72.216526
640.839152	0.178216	72.221530
640.283686	-1.630295	72.226535
639.969437	-6.241507	72.231540
638.670766	6.569423	72.236545
638.360859	-4.614965	72.241550
637.803931	-4.193519	72.246554
636.762609	4.829737	72.251559
635.941990	2.655035	72.256564
635.187647	-2.479008	72.261569
635.089250	-1.064599	72.266574
634.325898	-2.409514	72.271578
633.637536	-6.352470	72.276583
633.033177	-3.113450	72.281588
632.074361	1.840904	72.286593
631.946894	-0.803707	72.291598
630.570109	-0.272202	72.296602
630.201359	-1.214770	72.301607
630.227811	-6.402185	72.306612
629.209199	-3.330578	72.311617
628.525727	-6.008068	72.316622
627.840027	-4.071221	72.321626
626.669148	-2.154879	72.326631
626.084634	-3.033125	72.331636
625.286679	2.490103	72.336641
625.402067	-5.471034	72.341646
624.624385	-1.056435	72.346650
623.406275	-1.542060	72.351655
622.699306	0.592134	72.356660
622.079720	15.876307	72.361665
621.991910	1.264655	72.366670
621.036222	-0.869610	72.371674
620.089419	-11.520496	72.376679
619.838442	10.179682	72.381684
619.238854	-13.449120	72.386689
618.308768	17.192953	72.391694
617.528813	-13.121535	72.396698
616.932574	23.558913	72.401703
616.786053	-4.461164	72.406708
615.554102	-2.367941	72.411713
614.749226	-4.764330	72.416718
614.260972	6.455773	72.421722
613.895697	-13.250766	72.426727
613.270183	13.542494	72.431732
612.293687	8.497448	72.436737
611.757708	-6.624697	72.441742
611.556749	17.013408	72.446746
610.496549	-14.119004	72.451751
609.825547	3.920288	72.456756
609.269526	-1.786202	72.461761
608.895912	-12.536248	72.466766
607.793833	7.482888	72.471770
607.153072	-9.177380	72.476775
606.977145	-3.724825	72.481780
605.521669	6.662178	72.486785
604.948838	-0.680024	72.491790
604.342526	-5.385061	72.496794
603.610405	-0.755370	72.501799
603.655605	-5.989923	72.506804
602.108452	-8.332749	72.511809
601.514883	-0.262272	72.516814
601.075063	7.938258	72.521818
600.748397	2.550044	72.526823
600.682268	-7.891017	72.531828
599.048204	3.112608	72.536833
598.589965	2.237911	72.541838
598.281441	0.200856	72.546842
596.952858	0.980158	72.551847
596.409243	-8.643720	72.556852
595.721438	1.663604	72.561857
595.793255	0.490035	72.566862
594.413408	-2.409267	72.571866
593.550785	5.193150	72.576871
593.627365	-3.198606	72.581876
592.744150	-5.082636	72.586881
591.655081	4.055466	72.591886
591.017283	-25.608285	72.596890
590.491390	4.543632	72.601895
590.228096	10.457944	72.606900
589.793941	1.501000	72.611905
588.750627	-20.425027	72.616910
588.274732	7.971742	72.621914
587.604710	-4.902477	72.626919
586.459111	-4.999101	72.631924
585.957838	6.371305	72.636929
585.727185	-6.328467	72.641934
584.643684	-8.007139	72.646938
583.889678	5.283169	72.651943
583.388927	-8.784902	72.656948
582.910674	-6.381208	72.661953
582.152024	-0.837422	72.666958
581.087170	-3.597655	72.671962
580.561330	5.569017	72.676967
580.287737	-4.941499	72.681972
579.213832	3.566590	72.686977
578.589009	1.191997	72.691982
577.790125	4.849926	72.696986
577.147433	3.667155	72.701991
577.237405	-6.533847	72.706996
575.992616	6.929242	72.712001
575.518821	0.151571	72.717006
575.212305	-2.380944	72.722010
574.325882	3.246271	72.727015
573.351621	-2.287945	72.732020
572.737603	7.365840	72.737025
572.350526	-6.255151	72.742030
571.428207	-0.461377	72.747034
570.475766	-5.735726	72.752039
570.030869	-6.949996	72.757044
569.188014	7.926627	72.762049
569.144273	12.907145	72.767054
568.516258	4.343766	72.772058
567.559946	9.898541	72.777063
567.098925	-10.022962	72.782068
566.233046	4.010534	72.787073
565.562128	-7.337100	72.792078
564.823347	-0.926032	72.797082
564.243326	6.590385	72.802087
563.795626	-2.673463	72.807092
562.914564	1.107939	72.812097
562.408207	-8.042488	72.817102
561.629035	-0.817618	72.822106
560.516641	-1.572351	72.827111
560.112218	-9.816531	72.832116
559.166205	2.416306	72.837121
559.207740	-3.451571	72.842126
558.783777	4.356944	72.847130
557.812644	-2.046630	72.852135
557.105882	-2.168982	72.857140
556.659213	7.997448	72.862145
555.607020	-6.241396	72.867150
554.999464	4.838446	72.872154
554.182618	-4.757672	72.877159
554.119719	-5.261683	72.882164
552.551123	9.727382	72.887169
552.037650	-13.237039	72.892174
551.732578	-12.945571	72.897178
551.080138	-5.332472	72.902183
550.605450	-5.692051	72.907188
549.833480	3.051798	72.912193
549.095533	-6.463847	72.917198
548.171231	1.343938	72.922202
547.140427	5.341578	72.927207
546.815727	7.036452	72.932212
546.422368	1.816559	72.937217
546.478188	-9.673625	72.942222
544.869528	-7.810516	72.947226
544.505911	3.550581	72.952231
544.386532	-3.822826	72.957236
542.847963	-9.505255	72.962241
542.386856	-4.510303	72.967246
541.553398	3.784466	72.972250
541.103024	-1.312806	72.977255
540.754000	3.978097	72.982260
539.598465	-1.410542	72.987265
539.130882	1.086074	72.992270
538.588459	9.739752	72.997274
537.652193	-3.661297	73.002279
536.964518	-1.725689	73.007284
536.087018	0.624916	73.012289
536.153591	-4.977300	73.017294
535.387072	-3.134785	73.022298
534.357822	6.052155	73.027303
533.654968	11.289038	73.032308
533.217101	20.563133	73.037313
532.949177	-0.850904	73.042318
531.725359	6.108923	73.047322
531.233783	-0.604405	73.052327
530.845457	7.575315	73.057332
529.771637	12.855519	73.062337
529.058811	4.889111	73.067342
528.385348	-1.084067	73.072346
527.922850	3.628848	73.077351
527.382490	0.595868	73.082356
526.414715	-5.617421	73.087361
525.928713	-7.189397	73.092366
525.604878	-0.563728	73.097370
524.183627	-2.491337	73.102375
523.595798	1.099873	73.107380
523.149119	7.751421	73.112385
522.835500	-4.788472	73.117390
522.306308	1.171347	73.122394
521.254555	-0.996459	73.127399
520.781108	-5.539716	73.132404
520.281062	-0.590595	73.137409
519.334096	-1.281777	73.142414
518.560892	-0.256597	73.147418
517.709901	-4.610410	73.152423
517.595044	-8.939559	73.157428
516.942610	-6.014544	73.162433
516.140481	-14.138592	73.167438
515.244273	-11.581583	73.172442
514.755349	-1.269660	73.177447
513.775710	2.005510	73.182452
513.044568	8.363340	73.187457
512.597604	-6.683063	73.192462
512.201611	-7.756884	73.197466
511.336442	3.269384	73.202471
510.782180	-5.710979	73.207476
509.949787	3.731604	73.212481
509.658322	-7.819949	73.217486
508.954666	3.757734	73.222490
507.656973	-7.649303	73.227495
507.298331	-8.604499	73.232500
506.875375	1.621228	73.237505
506.649518	-2.111522	73.242510
505.555874	-1.006911	73.247514
504.879035	11.872170	73.252519
504.552707	-3.527750	73.257524
503.214528	2.109948	73.262529
502.754108	2.572819	73.267534
502.282419	-0.836931	73.272538
501.432875	-1.065828	73.277543
500.683592	-13.946299	73.282548
499.290536	21.908613	73.287553
499.422825	-3.191279	73.292558
499.220372	-4.163470	73.297562
498.039479	15.858794	73.302567
497.494251	-6.723677	73.307572
496.748100	0.330375	73.312577
496.519419	-1.561695	73.317582
495.828711	6.521121	73.322586
494.677483	2.590441	73.327591
494.609390	-6.019525	73.332596
493.484689	5.324047	73.337601
492.905312	-6.153255	73.342606
492.059760	-3.713112	73.347610
491.620385	10.512650	73.352615
491.355880	2.534763	73.357620
489.740734	15.230597	73.362625
489.249632	-1.822460	73.367630
488.792028	12.929736	73.372634
488.615816	4.259720	73.377639
488.084404	-0.999665	73.382644
486.907865	3.948422	73.387649
486.441401	-2.363632	73.392654
485.520310	0.000241	73.397658
484.490619	-1.887223	73.402663
484.234537	-11.517445	73.407668
483.429624	-15.121675	73.412673
483.246764	7.237805	73.417678
482.434372	-4.741671	73.422682
481.554112	-5.058703	73.427687
481.303800	1.220956	73.432692
480.472855	7.512694	73.437697
479.907717	-5.737718	73.442702
479.004926	-10.087993	73.447706
478.337749	3.138037	73.452711
477.748931	-8.717784	73.457716
476.598809	10.553709	73.462721
476.001850	-6.204942	73.467726
475.686259	0.432032	73.472730
475.246381	-7.907399	73.477735
474.806297	-3.612772	73.482740
473.636744	-7.840128	73.487745
473.054942	-13.045747	73.492750
472.506691	7.303065	73.497754
471.543384	-1.378745	73.502759
471.110231	-2.639020	73.507764
470.547610	1.302985	73.512769
470.170873	-12.742222	73.517774
468.750882	5.261865	73.522778
468.376647	0.985077	73.527783
468.211497	-9.618377	73.532788
467.226567	-5.203837	73.537793
465.993507	-10.433432	73.542798
465.456232	-5.438951	73.547802
464.934531	3.064780	73.552807
464.843401	-1.414797	73.557812
463.998820	13.373819	73.562817
463.320544	-3.286723	73.567822
462.621415	-3.129578	73.572826
461.635362	-0.644966	73.577831
461.433003	2.022290	73.582836
460.385020	-0.201281	73.587841
460.151800	-3.745202	73.592846
459.352181	-0.367810	73.597850
458.471577	1.298946	73.602855
458.000249	-8.579245	73.607860
457.438037	-5.173446	73.612865
456.537211	-4.878515	73.617870
455.756590	-6.848221	73.622874
455.154285	-4.274939	73.627879
454.814237	-4.856213	73.632884
453.479486	-1.194878	73.637889
452.651580	-14.028111	73.642894
452.782505	-1.397566	73.647898
452.400336	3.953816	73.652903
451.585227	-11.011834	73.657908
450.245014	2.204734	73.662913
449.887435	-8.749667	73.667918
449.278077	-7.769493	73.672922
448.664819	-0.875369	73.677927
447.959221	-6.813437	73.682932
447.049253	0.039653	73.687937
446.572865	1.585246	73.692942
446.394932	-6.852679	73.697946
445.191828	0.715714	73.702951
444.812581	1.671844	73.707956
443.872034	1.922647	73.712961
443.719783	-7.238429	73.717966
442.825873	4.889947	73.722970
441.639371	2.134966	73.727975
441.723537	-0.628499	73.732980
440.751623	-8.247672	73.737985
440.067835	0.870064	73.742990
439.538168	-1.809797	73.747994
438.657558	-6.095784	73.752999
437.592743	-9.642823	73.758004
437.024024	1.288923	73.763009
436.144173	-4.121506	73.768014
436.401096	1.101249	73.773018
435.836730	-1.945228	73.778023
435.056793	-5.998105	73.783028
433.941044	-0.072551	73.788033
433.902707	0.477620	73.793038
432.696712	6.439633	73.798042
432.005005	-6.867863	73.803047
431.509285	-11.667734	73.808052
431.006773	3.679787	73.813057
430.247072	-10.052092	73.818062
429.216207	-0.891674	73.823066
428.384398	-0.189853	73.828071
428.365618	-5.868349	73.833076
427.633162	-2.969985	73.838081
426.341092	-9.374399	73.843086
426.162464	-4.402362	73.848090
425.562556	-0.332989	73.853095
425.302801	-7.915815	73.858100
424.141333	-7.721265	73.863105
423.610394	-9.609321	73.868110
422.983570	-0.456506	73.873114
422.167440	7.337237	73.878119
421.504227	-8.417392	73.883124
420.545538	-0.134180	73.888129
420.800229	-5.122994	73.893134
419.929605	6.438730	73.898138
419.105994	-6.423561	73.903143
418.418081	1.721897	73.908148
417.127828	1.321983	73.913153
416.870075	-0.649021	73.918158
416.094359	0.155825	73.923162
415.505631	5.827116	73.928167
415.572532	-6.514765	73.933172
414.412522	-3.475739	73.938177
413.855365	-8.683693	73.943182
413.152113	-6.811801	73.948186
411.925944	5.371099	73.953191
411.511644	-1.993147	73.958196
410.810141	-1.521809	73.963201
410.857506	-7.664985	73.968206
409.454122	4.598189	73.973210
408.582626	7.741054	73.978215
408.737024	0.745070	73.983220
407.576160	1.474097	73.988225
407.464754	-1.777003	73.993230
406.394282	3.625708	73.998234
405.398458	9.229406	74.003239
405.255108	1.429344	74.008244
404.310062	11.383470	74.013249
403.550823	-2.815237	74.018254
402.990461	6.754332	74.023258
402.636084	-1.467825	74.028263
401.615550	-2.711765	74.033268
400.607019	12.347401	74.038273
400.267954	1.869429	74.043278
399.921494	3.827973	74.048282
399.250009	6.934242	74.053287
398.849075	-3.382487	74.058292
397.822369	4.769652	74.063297
397.332873	5.509976	74.068302
395.867333	-1.119086	74.073306
395.283284	1.292036	74.078311
395.001781	4.586892	74.083316
394.729402	1.448171	74.088321
394.400367	-2.041053	74.093326
393.126125	-1.721291	74.098330
392.619016	6.031105	74.103335
392.256225	-0.480364	74.108340
391.005742	2.041678	74.113345
390.495703	-10.380148	74.118350
390.015709	-9.220309	74.123354
389.023748	-1.896841	74.128359
388.406391	-3.149826	74.133364
387.433156	1.676025	74.138369
387.152263	-2.082631	74.143374
386.864306	2.399072	74.148378
385.857637	2.493284	74.153383
385.235619	-2.756366	74.158388
384.400834	2.872137	74.163393
384.254940	0.192637	74.168398
382.991813	-2.636833	74.173402
382.358726	-3.407936	74.178407
381.868697	-1.773429	74.183412
381.295763	3.589434	74.188417
381.113748	-0.990767	74.193422
380.072721	3.210404	74.198426
379.410934	-2.069175	74.203431
378.828380	0.647628	74.208436
377.521661	-0.076057	74.213441
377.401563	-7.356290	74.218446
377.109011	4.119637	74.223450
376.038200	-5.598353	74.228455
375.393064	-6.529954	74.233460
374.573020	0.248907	74.238465
373.911389	-3.994681	74.243470
373.033983	-3.856409	74.248474
372.276667	0.234903	74.253479
371.911735	3.207178	74.258484
371.295598	-4.698881	74.263489
371.244433	4.236064	74.268494
370.240236	-1.698550	74.273498
369.143516	-7.777683	74.278503
369.195581	-2.597988	74.283508
367.951830	9.751730	74.288513
367.090665	1.345417	74.293518
366.684352	0.560258	74.298522
366.636705	4.166344	74.303527
365.818238	-6.135878	74.308532
364.706791	1.536208	74.313537
364.236873	-5.043333	74.318542
363.319466	-8.214875	74.323546
362.433110	-3.025985	74.328551
362.177848	3.700727	74.333556
361.675086	5.043966	74.338561
361.035244	-5.032839	74.343566
360.074327	-1.333262	74.348570
359.383020	0.104674	74.353575
359.128128	-7.261305	74.358580
357.800858	6.213427	74.363585
357.258657	-1.597183	74.368590
356.814490	0.854732	74.373594
356.257112	-1.186785	74.378599
355.863741	-4.298334	74.383604
354.726742	-0.868727	74.388609
354.322414	-10.759138	74.393614
353.792422	-8.733499	74.398618
352.544367	-6.880426	74.403623
352.227355	-7.500048	74.408628
351.420833	-4.991967	74.413633
350.744194	-12.169314	74.418638
350.196161	-7.406480	74.423642
349.449421	-4.371784	74.428647
349.061732	-13.599398	74.433652
348.424036	6.399405	74.438657
347.664263	-5.268284	74.443662
346.424412	-9.602637	74.448666
346.095474	-0.746429	74.453671
346.001179	-2.765548	74.458676
345.032519	-4.402490	74.463681
343.928797	-10.633451	74.468686
343.541311	-10.297287	74.473690
342.706450	-21.390048	74.478695
342.641182	-4.612595	74.483700
341.556372	-6.235756	74.488705
340.870116	-17.227627	74.493710
340.495249	-2.764584	74.498714
339.749628	2.349850	74.503719
338.978477	-17.850118	74.508724
338.170130	-7.531434	74.513729
337.731810	-2.765581	74.518734
337.473917	-9.211752	74.523738
336.458026	-9.346276	74.528743
336.088557	-6.735960	74.533748
335.155458	-3.066038	74.538753
334.042101	-17.958862	74.543758
333.572728	-10.428515	74.548762
332.807711	-2.944086	74.553767
332.879631	-11.869642	74.558772
331.633927	2.719570	74.563777
331.238533	-2.137265	74.568782
330.476991	-8.512634	74.573786
329.664897	-12.129856	74.578791
329.047813	-14.608107	74.583796
328.237996	-14.278750	74.588801
327.828150	-7.070111	74.593806
327.618625	-0.621913	74.598810
326.344671	-7.150576	74.603815
326.021165	-23.681496	74.608820
325.102421	-7.193793	74.613825
323.899163	-6.349167	74.618830
323.485720	-7.207296	74.623834
323.003766	-5.171960	74.628839
322.881107	-15.876767	74.633844
322.004214	-4.929016	74.638849
321.087935	-1.980828	74.643854
320.493061	0.099311	74.648858
319.852974	-1.917977	74.653863
319.584214	-2.920583	74.658868
317.967126	-2.598181	74.663873
317.482609	5.811338	74.668878
317.110354	-4.505207	74.673882
316.735941	-0.476480	74.678887
316.147566	-2.060480	74.683892
315.114401	-4.078197	74.688897
314.967992	-13.241757	74.693902
313.886779	-5.205483	74.698906
312.851584	8.184874	74.703911
312.446261	-25.842737	74.708916
311.933244	12.243561	74.713921
311.442020	-15.912247	74.718926
310.903577	0.406053	74.723930
309.847759	-9.065141	74.728935
309.306231	-11.441892	74.733940
308.593716	-4.541389	74.738945
307.680120	-0.595456	74.743950
307.182899	-11.027690	74.748954
306.624376	4.978439	74.753959
306.247883	-7.483567	74.758964
305.250504	7.764643	74.763969
304.725929	-10.427817	74.768974
304.538301	-2.649065	74.773978
303.196905	-3.863902	74.778983
302.657057	-11.204953	74.783988
301.660696	1.308772	74.788993
301.209797	-1.752600	74.793998
300.689217	-3.823620	74.799002
299.706672	2.544362	74.804007
299.423577	-6.207924	74.809012
298.632076	-7.516706	74.814017
298.340592	-6.014748	74.819022
297.525146	-5.485797	74.824026
296.528771	2.186897	74.829031
296.319319	2.445811	74.834036
295.600749	5.091274	74.839041
294.847283	4.017694	74.844046
294.227884	1.601317	74.849050
293.751090	7.052948	74.854055
292.918554	8.912364	74.859060
291.958581	-6.528418	74.864065
291.588049	-7.041735	74.869070
290.619779	7.329821	74.874074
289.618435	-3.228637	74.879079
289.504666	-11.359806	74.884084
288.790370	-0.370152	74.889089
288.436549	-2.813085	74.894094
287.688116	-0.377318	74.899098
286.767246	0.042289	74.904103
286.446541	-14.428087	74.909108
285.095831	-1.250783	74.914113
284.483376	-10.428366	74.919118
284.123967	-5.616740	74.924122
283.626266	2.039554	74.929127
283.542216	-6.821720	74.934132
282.255815	-6.148318	74.939137
281.242643	-7.300343	74.944142
280.706272	-2.550393	74.949146
279.691723	-2.828604	74.954151
278.907671	-10.323106	74.959156
278.363823	5.770569	74.964161
278.033931	-5.820533	74.969166
278.065262	-6.189750	74.974170
277.532231	-8.941570	74.979175
276.902857	-12.113254	74.984180
275.971941	6.103101	74.989185
274.960530	-11.176001	74.994190
274.320070	-4.912998	74.999194
273.476917	8.296958	75.004199
272.773123	-12.489282	75.009204
271.570066	-5.076942	75.014209
271.186943	-9.800106	75.019214
270.752530	-11.848583	75.024218
270.422471	-3.474722	75.029223
270.079915	-19.220459	75.034228
269.085667	-0.927788	75.039233
268.419846	-11.552323	75.044238
267.803909	-4.263522	75.049242
267.100294	-3.131092	75.054247
266.239353	-4.725249	75.059252
265.331297	-5.040927	75.064257
265.336234	-9.707676	75.069262
264.631489	0.537748	75.074266
263.285543	-4.240100	75.079271
262.977243	-5.435084	75.084276
262.697847	-8.597896	75.089281
261.913757	-2.351418	75.094286
260.843310	-6.282236	75.099290
260.198386	-11.603883	75.104295
259.893414	-4.298417	75.109300
259.284504	-2.676477	75.114305
258.055216	-5.768304	75.119310
257.628916	0.865828	75.124314
256.777056	6.517590	75.129319
257.026300	-7.908018	75.134324
256.147577	-3.371566	75.139329
255.404915	2.896697	75.144334
254.623024	4.647131	75.149338
253.718522	8.907011	75.154343
253.179209	2.292827	75.159348
252.348127	2.335452	75.164353
251.798770	2.337902	75.169358
250.976885	5.677905	75.174362
250.176611	5.802349	75.179367
250.185978	-1.886420	75.184372
249.480246	-3.554194	75.189377
248.204297	0.233483	75.194382
247.814913	-2.279465	75.199386
247.257924	6.855942	75.204391
246.796896	2.203541	75.209396
245.352673	-2.216448	75.214401
244.970783	2.379581	75.219406
244.684306	-5.987395	75.224410
244.043530	-7.633983	75.229415
243.433438	-5.340099	75.234420
242.636259	0.003340	75.239425
242.286571	-1.134584	75.244430
241.197182	0.508757	75.249434
240.186756	5.512469	75.254439
239.910812	-10.188696	75.259444
239.195434	-10.684881	75.264449
238.831683	-1.570819	75.269454
237.799609	-14.163255	75.274458
237.525754	0.185922	75.279463
236.913858	-10.729459	75.284468
235.297039	-1.904490	75.289473
234.756312	-3.801980	75.294478
234.564830	-13.404600	75.299482
233.704610	-7.160173	75.304487
233.923954	-13.240870	75.309492
232.842377	9.873658	75.314497
231.627531	-2.427887	75.319502
231.276571	-4.052864	75.324506
230.596163	-7.042943	75.329511
230.639954	-15.238639	75.334516
229.436331	-8.849590	75.339521
228.837565	-0.248397	75.344526
227.939696	-2.082647	75.349530
226.614459	0.452966	75.354535
226.586539	-12.230150	75.359540
225.895620	0.742662	75.364545
225.386831	0.934185	75.369550
225.205670	-14.447780	75.374554
224.061522	-7.096849	75.379559
223.762255	-20.608719	75.384564
222.826979	3.543721	75.389569
221.935163	-9.859510	75.394574
221.211714	-13.965464	75.399578
220.715477	2.894869	75.404583
220.406312	-7.904770	75.409588
219.564017	-6.546802	75.414593
218.309552	4.476938	75.419598
218.341764	-7.085141	75.424602
217.748626	-0.787093	75.429607
217.128246	-12.234100	75.434612
216.090774	-4.092806	75.439617
215.531412	-19.442858	75.444622
214.470839	-7.022955	75.449626
213.573012	-5.082148	75.454631
213.165800	-9.938648	75.459636
212.817891	-5.045274	75.464641
212.607710	-12.088782	75.469646
212.196027	-5.247252	75.474650
210.814683	2.612989	75.479655
210.599819	-5.937276	75.484660
209.486465	1.672095	75.489665
208.536895	-12.617590	75.494670
207.980490	-10.266028	75.499674
207.304059	-3.114223	75.504679
207.387518	-11.174324	75.509684
206.170423	-7.414933	75.514689
205.353335	-18.289702	75.519694
205.081985	-17.473736	75.524698
204.317531	-13.411206	75.529703
203.611321	-13.982955	75.534708
202.400193	-13.062903	75.539713
202.700302	-19.869223	75.544718
202.304464	-8.709564	75.549722
200.906028	-7.993030	75.554727
200.452336	-13.676288	75.559732
199.705210	-10.009162	75.564737
198.760964	-2.748431	75.569742
198.324494	-6.236262	75.574746
197.506255	-9.146013	75.579751
197.108492	-2.423389	75.584756
195.992280	-6.296420	75.589761
195.369971	-9.745162	75.594766
194.879849	-4.463277	75.599770
194.638024	-9.007110	75.604775
194.267674	-2.005017	75.609780
192.919419	-4.653662	75.614785
192.745109	-15.589899	75.619790
191.605802	-13.919658	75.624794
190.382914	0.066748	75.629799
190.162685	-6.450055	75.634804
189.465750	-1.288156	75.639809
189.269145	-3.024462	75.644814
188.820890	-16.886295	75.649818
187.782795	-3.776138	75.654823
187.166691	-6.732302	75.659828
186.608566	-7.786528	75.664833
185.235005	-5.165922	75.669838
185.013287	-13.101678	75.674842
184.163163	1.691012	75.679847
184.158961	-10.029251	75.684852
183.082558	-6.437352	75.689857
182.131299	3.022678	75.694862
182.056413	-14.700545	75.699866
181.077014	-5.619215	75.704871
180.586109	-7.676014	75.709876
179.557734	-10.426108	75.714881
178.945516	-5.689280	75.719886
178.790398	-10.026170	75.724890
178.050638	-5.040360	75.729895
177.169876	-18.746507	75.734900
176.263158	3.195329	75.739905
175.989375	-14.338496	75.744910
175.471097	-10.542275	75.749914
173.978615	-10.723747	75.754919
173.927101	-4.846341	75.759924
173.634369	-7.185458	75.764929
172.508555	-6.039306	75.769934
171.668080	-4.517618	75.774938
170.922858	-4.717301	75.779943
170.921270	-5.645795	75.784948
170.357306	2.252878	75.789953
169.656511	-3.788355	75.794958
169.091516	0.762760	75.799962
167.662542	-11.947703	75.804967
166.738166	-16.008989	75.809972
166.172894	-1.184445	75.814977
165.913662	-12.461939	75.819982
165.706426	-10.330032	75.824986
164.444196	-15.040743	75.829991
164.048561	-8.933442	75.834996
163.266287	-5.782650	75.840001
162.666333	-17.056278	75.845006
161.845163	-11.500848	75.850010
160.763234	-5.405548	75.855015
160.476156	-2.743694	75.860020
160.251035	-12.834501	75.865025
159.657412	-14.010787	75.870030
158.931457	-12.572006	75.875034
157.971818	-2.443615	75.880039
157.710992	-16.196555	75.885044
156.266644	-6.653177	75.890049
155.847329	-7.650682	75.895054
155.330798	-14.984366	75.900058
154.810062	-1.196625	75.905063
154.459699	-20.623100	75.910068
153.277237	-8.372973	75.915073
152.647483	-6.380272	75.920078
152.294571	-8.414914	75.925082
150.981330	0.448431	75.930087
150.778679	-14.163724	75.935092
150.200738	-7.081226	75.940097
149.726241	-10.473100	75.945102
149.168099	-7.572494	75.950106
148.105569	-14.733972	75.955111
147.719924	-15.087168	75.960116
146.327512	-16.475123	75.965121
145.713930	-25.414359	75.970126
144.919304	-25.506814	75.975130
144.525963	-14.185136	75.980135
144.721842	-34.092902	75.985140
143.989835	-15.985532	75.990145
142.815049	-9.079097	75.995150
142.557509	-24.076709	76.000154
141.563180	-16.511529	76.005159
140.595876	-16.699448	76.010164
139.970837	-19.300951	76.015169
139.762719	-24.373669	76.020174
139.039733	-13.748450	76.025178
137.894876	-15.254715	76.030183
137.587144	-19.321271	76.035188
137.102508	-19.570376	76.040193
136.295408	-16.658459	76.045198
135.580060	-28.637458	76.050202
134.857721	-10.355011	76.055207
134.410257	-15.296534	76.060212
133.448292	-21.035920	76.065217
132.678370	-24.036923	76.070222
132.132005	-31.498292	76.075226
131.511015	-16.824143	76.080231
131.617019	-28.388499	76.085236
130.277466	-17.441056	76.090241
129.613712	-19.065025	76.095246
129.390402	-23.214421	76.100250
128.221798	-9.503151	76.105255
127.373213	-25.984976	76.110260
127.141779	-22.732780	76.115265
126.308378	-22.888429	76.120270
125.356271	-17.668490	76.125274
124.559913	-10.033947	76.130279
124.693496	-25.300488	76.135284
124.055933	-22.327295	76.140289
123.096039	-16.344479	76.145294
122.469158	-24.630335	76.150298
121.776991	-21.235293	76.155303
120.926640	-23.919130	76.160308
120.103995	-13.278017	76.165313
119.373677	-18.412543	76.170318
119.199490	-25.696723	76.175322
118.516456	-10.310961	76.180327
117.906604	-12.416586	76.185332
116.871334	-7.661175	76.190337
116.360497	-22.159521	76.195342
116.221404	-17.487087	76.200346
114.912822	-21.282093	76.205351
114.589430	-17.512208	76.210356
114.037085	-1.052920	76.215361
112.893797	-24.265185	76.220366
112.321362	-20.360977	76.225370
111.121132	-11.335877	76.230375
111.269064	-12.729737	76.235380
110.578776	-17.008090	76.240385
109.588332	-16.194142	76.245390
109.021991	-12.899578	76.250394
108.325110	-10.856742	76.255399
108.198412	-20.036022	76.260404
107.208334	-8.690147	76.265409
106.333036	-10.291416	76.270414
106.059725	-24.624213	76.275418
105.157274	-14.560126	76.280423
104.284250	-19.585162	76.285428
103.454712	-9.400239	76.290433
103.191329	-15.422886	76.295438
103.399986	-9.320478	76.300442
101.818199	-13.011994	76.305447
101.482530	-18.851233	76.310452
100.856388	-15.812050	76.315457
99.792726	-13.292853	76.320462
99.100886	-20.041924	76.325466
98.374491	-8.829552	76.330471
98.114873	-9.485098	76.335476
96.791512	-12.727409	76.340481
96.159422	-14.156153	76.345486
95.967275	-16.293687	76.350490
95.046090	-15.823498	76.355495
94.996229	-18.549820	76.360500
93.829896	-10.275982	76.365505
93.191513	-23.033603	76.370510
92.665083	-17.449466	76.375514
92.074370	-13.972826	76.380519
91.592682	-14.749071	76.385524
90.639552	-8.828819	76.390529
90.292772	-16.214782	76.395534
89.275788	-11.810768	76.400538
88.395707	-9.667753	76.405543
88.134344	-24.847658	76.410548
87.462838	-21.772855	76.415553
87.112950	-10.924859	76.420558
86.317666	-5.796138	76.425562
85.661673	-11.470762	76.430567
84.512650	-30.527001	76.435572
83.503150	-4.226052	76.440577
83.138191	-18.437007	76.445582
82.775231	-23.388836	76.450586
82.135540	-18.113050	76.455591
81.626672	-23.103110	76.460596
80.928789	-23.005977	76.465601
80.166479	-19.874116	76.470606
79.362294	-22.078044	76.475610
77.889922	-11.768530	76.480615
77.468711	-20.568118	76.485620
77.200199	-17.510269	76.490625
76.952370	-18.766906	76.495630
76.751416	-29.626325	76.500634
75.948090	-13.447133	76.505639
74.953387	-15.609640	76.510644
74.582793	-20.016228	76.515649
73.362074	-17.505090	76.520654
72.950613	-20.173746	76.525658
72.250221	-13.749770	76.530663
71.351467	-16.306028	76.535668
70.131278	-15.780264	76.540673
69.536908	-13.979259	76.545678
69.460731	-14.894279	76.550682
69.095072	-14.471671	76.555687
69.033598	-19.239776	76.560692
67.928071	-17.995893	76.565697
67.106054	-12.720987	76.570702
66.297843	-24.670959	76.575706
65.320209	-10.822975	76.580711
65.144520	-19.403105	76.585716
63.999448	-13.464852	76.590721
63.030207	-20.906076	76.595726
62.618548	-23.224631	76.600730
61.829314	-2.473146	76.605735
61.563923	-22.520234	76.610740
61.383102	-23.317645	76.615745
60.721719	-19.407127	76.620750
59.908641	-12.867411	76.625754
59.100876	-13.143815	76.630759
58.374273	-22.162764	76.635764
57.416846	-21.648937	76.640769
56.740000	-23.756474	76.645774
56.443291	-7.388419	76.650778
55.605014	-11.756690	76.655783
54.741374	-13.303030	76.660788
54.370839	-6.658852	76.665793
53.794116	-22.890696	76.670798
52.933366	-12.833244	76.675802
51.984979	-12.445429	76.680807
51.887153	-19.844277	76.685812
51.444654	-7.313170	76.690817
50.136505	-7.098206	76.695822
49.694555	-15.041390	76.700826
48.773131	-7.576108	76.705831
48.402042	-7.434892	76.710836
47.768151	-9.465705	76.715841
46.865607	-10.938033	76.720846
46.631591	-24.438181	76.725850
46.157614	-13.310211	76.730855
45.492618	-13.634609	76.735860
44.332222	-11.235573	76.740865
43.666123	-18.469679	76.745870
42.734587	-16.496632	76.750874
41.622153	-9.365145	76.755879
41.461115	-19.216997	76.760884
41.096718	-10.763541	76.765889
40.621882	-11.812091	76.770894
40.532620	-14.979961	76.775898
38.979266	-5.340297	76.780903
38.773297	-9.738444	76.785908
37.949005	-6.878945	76.790913
36.904641	-7.038764	76.795918
36.199413	-17.557575	76.800922
35.558259	-13.405860	76.805927
35.466425	-17.582521	76.810932
34.490236	-9.263294	76.815937
33.678109	-0.235401	76.820942
33.287421	1.421171	76.825946
32.968641	-8.861247	76.830951
32.202287	-6.548702	76.835956
31.178418	-14.361230	76.840961
30.498402	-12.686899	76.845966
29.466811	-19.829594	76.850970
28.526170	-10.047961	76.855975
28.284953	-12.586074	76.860980
27.863731	-6.389527	76.865985
27.492657	-11.092485	76.870990
27.176947	-17.411110	76.875994
26.094144	-10.770023	76.880999
25.383713	-18.227276	76.886004
24.839553	-8.699678	76.891009
23.225014	-9.214812	76.896014
23.137802	-16.697348	76.901018
22.765715	-12.479738	76.906023
22.371104	-13.422813	76.911028
20.966437	-8.958519	76.916033
20.435010	-10.100537	76.921038
19.875890	-14.710426	76.926042
19.205160	1.223727	76.931047
19.159560	-14.052081	76.936052
17.927129	0.847343	76.941057
17.532883	-10.449583	76.946062
17.360391	-12.722702	76.951066
16.035223	-0.940170	76.956071
15.594752	-8.490941	76.961076
14.601715	-0.203708	76.966081
13.543455	-3.581289	76.971086
12.832348	-1.315395	76.976090
12.401055	-6.795610	76.981095
12.462446	-1.237401	76.986100
11.672711	-14.882294	76.991105
10.560247	-14.673289	76.996110
10.409448	-9.284658	77.001114
9.516592	-20.133060	77.006119
8.735680	-29.930184	77.011124
7.724496	-2.663906	77.016129
7.379852	-9.266485	77.021134
7.021565	-8.701548	77.026139
6.143642	-10.220363	77.031143
5.526449	-12.685892	77.036148
5.028626	-22.906622	77.041153
4.360568	-13.362417	77.046158