Mon Mar 08 18:32:20 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.217972	100.852660	0.000000
0.415817	81.214133	0.005005
-0.722085	61.755585	0.010010
-1.597932	2.374427	0.015014
-5.428840	-44.107801	0.020019
-11.171586	-34.476346	0.025024
-16.366299	-40.048193	0.030029
-21.375295	-30.983168	0.035034
-25.572141	-38.683688	0.040038
-28.819203	-43.590113	0.045043
-33.069019	-35.694793	0.050048
-36.223826	-41.462706	0.055053
-40.264208	-42.588950	0.060058
-43.496515	-32.492202	0.065062
-47.428064	-23.975878	0.070067
-51.249033	-23.348935	0.075072
-55.085473	-38.365241	0.080077
-58.836260	-28.428595	0.085082
-62.491703	-29.086385	0.090086
-66.103842	-32.644638	0.095091
-70.037546	-22.281418	0.100096
-73.797146	-47.400345	0.105101
-77.704731	-28.426842	0.110106
-81.778102	-14.412934	0.115110
-85.105834	-38.455948	0.120115
-89.102473	-36.108936	0.125120
-92.527627	-44.703541	0.130125
-96.454187	-23.107798	0.135130
-100.219222	-22.887074	0.140134
-104.087094	-28.550590	0.145139
-107.621783	-31.216013	0.150144
-111.252530	-39.009854	0.155149
-115.121986	-33.191902	0.160154
-119.032116	-20.746169	0.165158
-122.751101	-40.264141	0.170163
-127.101499	-29.804391	0.175168
-130.439353	-44.099064	0.180173
-134.326291	-15.829961	0.185178
-138.107205	-38.923833	0.190182
-141.574203	-27.512249	0.195187
-145.403239	-15.371133	0.200192
-149.216437	-30.734749	0.205197
-152.818382	-37.500271	0.210202
-156.934970	-20.633108	0.215206
-160.333695	-28.556938	0.220211
-164.614261	-39.876952	0.225216
-167.802102	-18.935123	0.230221
-171.809092	-31.364753	0.235226
-175.478444	-17.158149	0.240230
-178.960075	-37.213772	0.245235
-182.982718	-19.273520	0.250240
-186.587149	-35.553429	0.255245
-190.670209	-36.002441	0.260250
-194.429228	-33.399881	0.265254
-198.020310	-31.434365	0.270259
-202.155858	-22.877363	0.275264
-205.528622	-41.378171	0.280269
-209.225586	-27.998133	0.285274
-212.839163	-18.281842	0.290278
-216.535088	-40.465086	0.295283
-220.597050	-15.091450	0.300288
-224.158735	-39.415421	0.305293
-228.644640	-36.548570	0.310298
-232.278660	-24.436884	0.315302
-235.617847	-31.367213	0.320307
-239.313013	-35.334548	0.325312
-242.925155	-27.744069	0.330317
-247.080605	-26.054234	0.335322
-250.463788	-31.884749	0.340326
-254.266602	-47.252973	0.345331
-258.294956	-33.041005	0.350336
-261.989133	-35.073645	0.355341
-265.970185	-34.605305	0.360346
-269.731665	-43.325721	0.365350
-273.245766	-40.935591	0.370355
-277.489790	-17.450287	0.375360
-280.884102	-45.618465	0.380365
-284.543975	-8.029848	0.385370
-288.112431	-46.347331	0.390374
-292.291621	-11.378564	0.395379
-295.896687	-37.977217	0.400384
-299.498256	-17.073270	0.405389
-303.394968	-26.325535	0.410394
-307.479520	-32.383027	0.415398
-310.683925	-23.876729	0.420403
-314.820613	-4.456303	0.425408
-318.277160	-38.441029	0.430413
-322.347778	-14.702654	0.435418
-325.649867	-41.250273	0.440422
-329.333992	-37.224515	0.445427
-334.086536	-25.082346	0.450432
-337.591060	-35.767455	0.455437
-341.347870	-23.908813	0.460442
-344.726535	-24.261874	0.465446
-348.500286	-35.375467	0.470451
-352.362968	-35.189219	0.475456
-356.206598	-30.650702	0.480461
-359.716409	-31.186219	0.485466
-363.209146	-26.850362	0.490470
-367.121093	-22.327725	0.495475
-371.067915	-22.296738	0.500480
-374.436125	-38.530469	0.505485
-378.725130	-26.282467	0.510490
-382.462555	-18.726972	0.515494
-386.079815	-31.565353	0.520499
-390.345898	-33.883347	0.525504
-393.674890	-29.240875	0.530509
-397.823871	-26.309245	0.535514
-400.977084	-24.671952	0.540518
-405.066306	-28.736945	0.545523
-409.096025	-24.892412	0.550528
-412.547998	-35.024429	0.555533
-416.113651	-31.798007	0.560538
-419.935684	-35.071475	0.565542
-423.400880	-39.403228	0.570547
-427.587319	-40.641104	0.575552
-431.677927	-33.978417	0.580557
-435.077452	-34.589778	0.585562
-438.963272	-25.972928	0.590566
-442.308929	-35.751313	0.595571
-446.321194	-30.895583	0.600576
-450.067903	-36.864855	0.605581
-453.996623	-37.156725	0.610586
-457.640811	-31.807856	0.615590
-461.285146	-38.307515	0.620595
-465.610824	-7.673561	0.625600
-468.953807	-31.450179	0.630605
-472.889467	-27.683637	0.635610
-476.655847	-19.785930	0.640614
-480.202299	-35.611004	0.645619
-484.015241	-17.968711	0.650624
-487.746036	-37.815297	0.655629
-491.288035	-26.911638	0.660634
-495.348714	-41.730508	0.665638
-498.654988	-35.590352	0.670643
-502.945352	-24.770564	0.675648
-506.908147	-24.755724	0.680653
-510.721780	-32.977009	0.685658
-514.121236	-31.729146	0.690662
-517.588240	-27.006118	0.695667
-521.833922	-31.589933	0.700672
-524.905198	-38.244098	0.705677
-528.824072	-34.078049	0.710682
-532.925892	-37.300334	0.715686
-536.463489	-36.057181	0.720691
-540.624124	-20.674108	0.725696
-544.078181	-25.922044	0.730701
-547.975934	-32.090945	0.735706
-551.779541	-34.086728	0.740710
-555.369008	-27.997445	0.745715
-559.308834	-26.101835	0.750720
-563.317766	-26.841156	0.755725
-567.181106	-21.944365	0.760730
-570.610932	-21.271855	0.765734
-573.900613	-22.659037	0.770739
-578.164145	-20.563458	0.775744
-581.651591	-38.428787	0.780749
-585.545179	-22.285684	0.785754
-589.521077	-35.175233	0.790758
-593.080312	-23.196413	0.795763
-596.812342	-20.438279	0.800768
-600.531568	-36.916755	0.805773
-604.417595	-6.926811	0.810778
-607.945891	-22.874429	0.815782
-611.728174	-30.034594	0.820787
-616.200887	-29.072407	0.825792
-619.648701	-29.675788	0.830797
-623.285806	-25.450531	0.835802
-627.086135	-32.664552	0.840806
-630.225396	-20.385370	0.845811
-634.415627	-38.565654	0.850816
-638.311254	-24.218194	0.855821
-641.822998	-23.515148	0.860826
-645.830140	-27.906627	0.865830
-649.194035	-39.663897	0.870835
-653.476680	-9.665713	0.875840
-656.859239	-51.443429	0.880845
-660.892157	-16.059177	0.885850
-664.755277	-63.165541	0.890854
-668.492606	-5.236829	0.895859
-672.210504	-16.872865	0.900864
-675.589792	-40.867234	0.905869
-679.559973	-27.617912	0.910874
-683.609441	-23.443359	0.915878
-687.035973	-32.763776	0.920883
-691.158694	-20.992804	0.925888
-694.302661	-39.466308	0.930893
-698.651868	-33.255414	0.935898
-702.230484	-21.459415	0.940902
-705.645414	-28.066305	0.945907
-709.408299	-34.567122	0.950912
-713.419841	-44.916726	0.955917
-717.211553	-26.914831	0.960922
-721.087717	-21.124821	0.965926
-724.973247	-32.691389	0.970931
-728.714115	-27.749267	0.975936
-731.938856	-38.341271	0.980941
-735.698094	-21.115617	0.985946
-739.651342	-39.212148	0.990950
-743.459574	-37.696792	0.995955
-747.728833	-29.272061	1.000960
-751.123085	-28.743741	1.005965
-755.152821	-29.036312	1.010970
-758.864421	-32.927657	1.015974
-762.110050	-33.881670	1.020979
-766.176239	-24.767160	1.025984
-769.811108	-34.637587	1.030989
-773.742175	-29.825836	1.035994
-777.422172	-49.057144	1.040998
-780.917264	-23.825369	1.046003
-784.847553	-23.326433	1.051008
-788.574744	-29.104316	1.056013
-792.618804	-26.616108	1.061018
-796.253789	-27.835826	1.066022
-799.593896	-30.532883	1.071027
-803.904039	-30.462024	1.076032
-807.626147	-43.085824	1.081037
-811.641084	-38.676898	1.086042
-815.078632	-23.596623	1.091046
-818.681786	-36.701445	1.096051
-822.562766	-22.554735	1.101056
-826.091471	-42.052987	1.106061
-830.074470	-42.468011	1.111066
-833.961191	-20.309929	1.116070
-837.300354	-25.361334	1.121075
-841.262531	-32.404049	1.126080
-844.996760	-32.299033	1.131085
-848.804594	-43.634956	1.136090
-852.892846	-16.363992	1.141094
-856.371796	-23.405094	1.146099
-860.397338	-33.485712	1.151104
-863.951467	-29.913565	1.156109
-867.548726	-21.788435	1.161114
-871.463512	-26.055522	1.166118
-875.269343	-34.334199	1.171123
-879.236981	-26.411598	1.176128
-882.737838	-24.746475	1.181133
-886.571712	-25.358701	1.186138
-890.213595	-35.169463	1.191142
-893.873059	-29.148917	1.196147
-897.875327	-17.832079	1.201152
-901.491373	-33.388294	1.206157
-905.178389	-26.555975	1.211162
-909.213850	-25.327277	1.216166
-913.074126	-43.198659	1.221171
-916.535048	-21.411301	1.226176
-920.357568	-29.133758	1.231181
-924.070990	-16.786069	1.236186
-927.776945	-24.114018	1.241190
-931.268720	-30.503284	1.246195
-935.274831	-23.739737	1.251200
-938.800949	-36.252738	1.256205
-942.918526	-35.657363	1.261210
-946.796541	-16.545416	1.266214
-950.180644	-36.659483	1.271219
-954.072109	-38.244768	1.276224
-958.069786	-27.321213	1.281229
-962.067334	-31.016700	1.286234
-965.959109	-38.880954	1.291238
-969.316803	-38.539504	1.296243
-973.051738	-34.028438	1.301248
-976.800647	-20.353596	1.306253
-980.413991	-37.761333	1.311258
-984.339309	-32.904432	1.316262
-988.005738	-38.961341	1.321267
-991.863262	-29.302708	1.326272
-995.391155	-22.092025	1.331277
-999.310564	-37.653164	1.336282
-1003.120120	-30.742759	1.341286
-1006.653905	-20.210259	1.346291
-1010.733894	-42.745353	1.351296
-1014.493942	-34.833663	1.356301
-1018.045963	-32.709179	1.361306
-1021.802228	-46.022535	1.366310
-1025.599202	-29.137354	1.371315
-1029.547025	-33.075628	1.376320
-1033.165754	-31.482889	1.381325
-1036.395647	-58.928586	1.386330
-1040.973022	-21.411587	1.391334
-1044.523985	-47.744714	1.396339
-1048.646728	-38.914001	1.401344
-1052.205829	-48.930100	1.406349
-1055.815079	-25.407966	1.411354
-1059.730244	-23.827690	1.416358
-1063.195600	-36.662422	1.421363
-1066.848640	-37.585532	1.426368
-1070.450762	-23.006847	1.431373
-1074.275386	-33.787797	1.436378
-1078.694776	-33.979637	1.441382
-1081.917239	-31.945618	1.446387
-1086.240217	-25.706689	1.451392
-1089.519210	-46.017084	1.456397
-1093.563169	-25.329923	1.461402
-1096.987416	-27.235698	1.466406
-1100.739585	-51.660073	1.471411
-1104.855643	-12.427025	1.476416
-1108.226089	-40.632270	1.481421
-1112.116466	-29.099626	1.486426
-1115.788763	-40.031016	1.491430
-1119.926985	-43.104514	1.496435
-1123.545661	-26.667156	1.501440
-1127.345597	-28.585318	1.506445
-1131.182522	-39.966553	1.511450
-1134.883681	-29.422872	1.516454
-1138.439170	-27.789629	1.521459
-1142.454148	-27.934093	1.526464
-1145.781166	-29.169420	1.531469
-1149.653286	-31.359829	1.536474
-1153.755569	-30.017525	1.541478
-1157.644712	-38.872125	1.546483
-1161.372415	-23.398070	1.551488
-1164.511997	-22.091512	1.556493
-1168.213908	-44.169571	1.561498
-1172.329850	-15.121334	1.566502
-1175.478697	-35.834025	1.571507
-1179.901678	-33.644052	1.576512
-1183.947750	-32.061547	1.581517
-1187.631278	-31.260820	1.586522
-1191.194382	-32.822557	1.591526
-1194.629135	-34.180914	1.596531
-1198.847111	-33.999503	1.601536
-1202.472114	-32.459113	1.606541
-1206.356866	-28.628563	1.611546
-1209.943936	-29.527312	1.616550
-1213.609988	-39.448773	1.621555
-1217.656288	-39.498213	1.626560
-1221.576894	-26.809460	1.631565
-1225.043399	-24.969567	1.636570
-1228.954789	-34.399188	1.641574
-1232.372805	-27.929526	1.646579
-1236.278537	-22.488756	1.651584
-1239.952579	-45.854697	1.656589
-1243.623869	-10.030824	1.661594
-1247.552088	-47.755886	1.666598
-1251.279087	-7.386487	1.671603
-1255.224729	-35.352783	1.676608
-1258.570781	-14.094273	1.681613
-1262.517378	-41.475378	1.686618
-1266.840452	-23.135362	1.691622
-1270.205917	-24.233477	1.696627
-1274.087791	-22.757514	1.701632
-1277.574224	-24.938477	1.706637
-1281.193747	-33.064933	1.711642
-1285.184183	-26.937214	1.716646
-1288.578975	-37.509052	1.721651
-1292.646941	-39.885476	1.726656
-1296.707164	-10.060696	1.731661
-1300.347483	-34.414320	1.736666
-1304.000661	-11.184414	1.741670
-1307.199026	-51.369360	1.746675
-1311.664340	-14.339762	1.751680
-1315.118583	-39.393296	1.756685
-1319.133520	-23.628627	1.761690
-1323.422407	-26.157282	1.766694
-1326.652692	-25.709564	1.771699
-1330.362872	-31.517651	1.776704
-1334.016699	-42.391702	1.781709
-1337.790735	-19.114034	1.786714
-1341.538941	-20.228044	1.791718
-1345.416114	-43.115029	1.796723
-1349.590562	-13.659801	1.801728
-1352.944303	-42.455448	1.806733
-1356.874591	-19.528032	1.811738
-1360.495541	-43.812094	1.816742
-1363.793126	-15.191031	1.821747
-1367.979282	-27.758505	1.826752
-1371.925030	-11.031901	1.831757
-1375.326904	-49.733444	1.836762
-1379.524800	-14.782263	1.841766
-1382.845152	-38.297608	1.846771
-1386.716553	-10.898162	1.851776
-1390.227522	-26.907147	1.856781
-1394.009607	-33.741182	1.861786
-1398.069991	-14.410158	1.866790
-1401.526412	-43.395845	1.871795
-1405.773989	-13.135670	1.876800
-1409.356102	-55.234771	1.881805
-1413.263431	-12.185649	1.886810
-1417.040943	-24.872069	1.891814
-1420.026691	-65.988034	1.896819
-1424.414715	-18.544555	1.901824
-1428.200742	-36.010586	1.906829
-1431.785111	-10.594979	1.911834
-1435.556096	-33.517729	1.916838
-1439.470040	-22.870141	1.921843
-1443.097470	-21.497710	1.926848
-1446.765154	-37.833131	1.931853
-1450.981463	-18.615826	1.936858
-1454.803620	-26.192346	1.941862
-1458.183092	-12.834552	1.946867
-1462.059074	-27.072509	1.951872
-1465.817470	-31.261110	1.956877
-1469.067285	-34.365854	1.961882
-1473.266451	-14.492132	1.966886
-1476.774826	-18.536264	1.971891
-1480.978800	-22.513151	1.976896
-1484.655064	-33.828029	1.981901
-1488.285015	-35.096341	1.986906
-1492.021740	-19.959383	1.991910
-1495.441364	-21.830610	1.996915
-1500.174642	-25.307197	2.006912
-1500.799730	-33.194504	2.016909
-1498.142425	-24.936228	2.026906
-1495.280629	-25.272883	2.036902
-1492.979121	-24.203036	2.046899
-1491.604766	-18.448628	2.056896
-1489.722518	-22.007185	2.066893
-1487.519562	-26.899137	2.076890
-1485.559279	-21.083827	2.086886
-1483.883990	-26.682288	2.096883
-1481.943962	-19.235919	2.106880
-1480.144978	-26.360425	2.116877
-1478.191524	-19.735635	2.126874
-1476.103983	-23.117066	2.136870
-1474.095654	-23.023357	2.146867
-1472.308317	-24.471545	2.156864
-1470.540549	-27.811238	2.166861
-1468.641236	-26.370662	2.176858
-1466.637891	-33.114216	2.186854
-1464.828642	-26.302123	2.196851
-1462.948020	-29.203589	2.206848
-1461.090408	-26.349559	2.216845
-1459.273873	-30.453329	2.226842
-1457.064494	-22.383788	2.236838
-1455.105999	-27.696016	2.246835
-1453.592889	-28.669249	2.256832
-1451.720322	-32.467790	2.266829
-1449.670316	-26.887858	2.276826
-1447.637216	-38.156453	2.286822
-1445.882987	-33.806462	2.296819
-1444.321284	-26.841036	2.306816
-1442.320956	-22.337821	2.316813
-1440.318791	-32.717296	2.326810
-1438.381085	-34.067962	2.336806
-1436.648773	-37.616677	2.346803
-1434.425204	-35.847485	2.356800
-1432.979460	-23.056413	2.366797
-1430.987968	-35.259340	2.376794
-1429.039170	-32.538300	2.386790
-1426.957280	-35.811418	2.396787
-1425.042263	-35.271695	2.406784
-1423.614822	-31.030407	2.416781
-1421.705222	-35.570606	2.426778
-1419.553155	-27.120818	2.436774
-1417.694732	-23.283247	2.446771
-1415.795552	-24.046704	2.456768
-1414.066402	-25.965507	2.466765
-1412.139302	-19.126447	2.476762
-1410.480192	-31.501924	2.486758
-1408.136241	-27.918915	2.496755
-1406.364522	-34.628494	2.506752
-1404.410913	-27.667366	2.516749
-1402.668391	-31.375579	2.526746
-1400.886521	-20.534512	2.536742
-1398.884153	-31.416070	2.546739
-1396.967805	-32.229625	2.556736
-1395.419137	-31.304400	2.566733
-1393.624799	-33.116788	2.576730
-1390.885994	-42.725251	2.586726
-1389.669461	-25.812925	2.596723
-1387.831934	-37.028061	2.606720
-1385.746420	-22.856820	2.616717
-1383.699408	-29.297843	2.626714
-1382.068733	-36.905304	2.636710
-1379.902548	-31.776516	2.646707
-1378.354565	-34.348359	2.656704
-1376.764596	-26.362723	2.666701
-1374.562571	-35.282112	2.676698
-1372.405651	-37.793549	2.686694
-1370.761216	-25.910510	2.696691
-1369.067295	-34.271736	2.706688
-1367.145309	-27.119204	2.716685
-1365.072314	-32.345483	2.726682
-1363.183912	-28.918436	2.736678
-1361.128753	-30.115744	2.746675
-1359.589388	-25.352355	2.756672
-1357.600194	-24.982337	2.766669
-1355.713045	-35.286495	2.776666
-1353.932785	-28.264414	2.786662
-1352.184275	-31.454102	2.796659
-1349.975130	-34.690686	2.806656
-1348.407539	-37.224598	2.816653
-1346.398310	-31.679092	2.826650
-1344.586975	-33.846251	2.836646
-1342.614254	-37.330757	2.846643
-1340.740651	-34.059209	2.856640
-1338.799036	-17.068703	2.866637
-1336.797259	-36.471272	2.876634
-1334.887066	-32.572450	2.886630
-1333.285086	-34.635039	2.896627
-1331.179556	-25.064608	2.906624
-1329.638882	-32.659211	2.916621
-1327.714384	-33.243499	2.926618
-1325.746467	-30.255442	2.936614
-1323.738613	-30.578347	2.946611
-1321.914513	-35.772643	2.956608
-1319.861440	-25.470683	2.966605
-1318.239687	-29.227397	2.976602
-1316.346014	-27.831578	2.986598
-1314.488417	-24.023785	2.996595
-1312.496940	-33.307297	3.006592
-1310.692409	-26.841667	3.016589
-1308.922719	-39.301091	3.026586
-1307.195321	-26.562901	3.036582
-1305.053722	-23.533153	3.046579
-1303.113449	-31.624311	3.056576
-1301.101563	-28.984305	3.066573
-1299.294922	-33.976853	3.076570
-1297.555977	-31.230003	3.086566
-1295.772398	-30.392833	3.096563
-1293.734319	-36.849717	3.106560
-1291.890033	-33.035041	3.116557
-1290.054126	-32.296237	3.126554
-1288.002507	-31.148294	3.136550
-1286.287489	-32.047951	3.146547
-1284.303797	-30.063384	3.156544
-1282.563148	-32.010773	3.166541
-1280.899605	-31.438575	3.176538
-1278.785942	-29.182715	3.186534
-1276.756705	-32.766208	3.196531
-1275.159953	-31.847018	3.206528
-1273.062792	-22.685693	3.216525
-1271.207066	-32.086388	3.226522
-1269.536743	-25.741341	3.236518
-1267.573713	-33.406661	3.246515
-1265.461679	-35.634515	3.256512
-1263.865530	-32.364285	3.266509
-1261.878119	-25.735259	3.276506
-1259.791515	-35.520246	3.286502
-1257.924868	-33.183783	3.296499
-1256.542893	-34.980597	3.306496
-1254.510660	-29.165542	3.316493
-1252.444164	-32.630247	3.326490
-1250.557981	-34.173029	3.336486
-1248.587377	-35.824052	3.346483
-1247.100138	-31.472221	3.356480
-1244.941109	-32.585003	3.366477
-1243.077224	-37.892971	3.376474
-1241.215815	-28.453902	3.386470
-1239.258577	-32.747385	3.396467
-1237.406705	-34.325717	3.406464
-1235.570606	-20.480697	3.416461
-1233.774650	-28.521869	3.426458
-1231.856325	-34.525350	3.436454
-1230.109409	-31.463950	3.446451
-1227.973465	-30.007358	3.456448
-1226.282850	-30.397827	3.466445
-1224.613549	-31.316963	3.476442
-1222.456602	-31.114192	3.486438
-1220.391209	-33.314019	3.496435
-1218.691158	-27.153681	3.506432
-1216.824939	-31.746777	3.516429
-1215.096632	-29.378668	3.526426
-1212.967771	-30.186607	3.536422
-1211.301178	-30.382178	3.546419
-1209.360475	-30.815811	3.556416
-1207.446770	-31.680891	3.566413
-1205.762887	-27.532595	3.576410
-1203.641677	-22.590632	3.586406
-1201.845354	-30.488162	3.596403
-1200.023173	-23.966843	3.606400
-1198.092437	-27.289785	3.616397
-1195.843710	-19.374679	3.626394
-1194.417065	-29.372947	3.636390
-1192.391338	-25.543010	3.646387
-1190.433518	-29.550773	3.656384
-1188.627591	-29.798621	3.666381
-1186.786863	-29.171026	3.676378
-1184.881012	-26.130283	3.686374
-1183.043699	-34.852212	3.696371
-1181.324797	-30.910017	3.706368
-1179.625953	-29.410282	3.716365
-1177.524160	-29.677042	3.726362
-1175.582725	-31.635954	3.736358
-1173.416200	-27.607486	3.746355
-1171.702911	-27.133164	3.756352
-1169.858104	-31.088093	3.766349
-1168.176627	-23.735851	3.776346
-1166.320301	-29.235179	3.786342
-1164.218814	-29.913963	3.796339
-1162.206862	-28.816400	3.806336
-1160.644650	-30.552001	3.816333
-1158.336365	-26.609354	3.826330
-1156.775374	-27.639002	3.836326
-1155.177189	-33.850140	3.846323
-1152.964539	-29.759562	3.856320
-1151.273518	-27.996461	3.866317
-1149.327527	-28.929814	3.876314
-1147.342133	-24.978125	3.886310
-1145.488116	-25.288894	3.896307
-1143.563706	-23.831535	3.906304
-1141.782745	-21.752831	3.916301
-1139.940550	-28.383509	3.926298
-1137.892988	-31.930347	3.936294
-1136.140498	-31.651735	3.946291
-1134.358950	-25.428582	3.956288
-1132.309321	-23.443378	3.966285
-1130.935585	-22.813654	3.976282
-1128.578634	-21.130233	3.986278
-1126.546538	-30.191168	3.996275
-1124.948149	-30.034729	4.006272
-1123.010670	-28.407347	4.016269
-1120.826697	-32.372291	4.026266
-1119.132889	-21.987389	4.036262
-1117.520901	-20.366348	4.046259
-1115.678755	-21.507261	4.056256
-1113.389020	-22.296638	4.066253
-1111.739066	-30.581197	4.076250
-1110.026259	-34.177085	4.086246
-1108.117601	-33.601345	4.096243
-1106.262553	-29.717185	4.106240
-1104.250629	-33.245662	4.116237
-1102.476180	-24.100433	4.126234
-1100.488448	-32.300079	4.136230
-1098.306358	-31.594396	4.146227
-1096.694448	-35.537274	4.156224
-1094.723146	-33.323203	4.166221
-1093.072188	-29.352702	4.176218
-1090.954206	-28.782013	4.186214
-1089.224437	-21.094816	4.196211
-1087.407736	-29.346039	4.206208
-1085.512209	-27.842960	4.216205
-1083.826684	-29.762440	4.226202
-1081.561462	-26.640154	4.236198
-1079.905139	-28.097087	4.246195
-1077.953058	-24.381574	4.256192
-1075.931692	-26.902639	4.266189
-1074.145214	-29.275609	4.276186
-1072.470483	-26.794614	4.286182
-1070.312938	-35.676631	4.296179
-1068.472813	-14.419284	4.306176
-1066.757169	-25.068429	4.316173
-1064.977580	-25.335651	4.326170
-1062.905145	-15.958586	4.336166
-1060.987816	-20.114501	4.346163
-1059.103984	-34.403000	4.356160
-1057.449616	-26.353210	4.366157
-1055.357369	-16.336705	4.376154
-1053.656100	-20.776988	4.386150
-1051.853545	-27.527572	4.396147
-1049.650002	-22.691783	4.406144
-1048.205642	-25.313156	4.416141
-1046.172321	-29.373931	4.426138
-1043.927041	-32.778638	4.436134
-1042.375779	-35.175537	4.446131
-1040.419125	-25.307854	4.456128
-1038.510547	-30.308626	4.466125
-1036.800994	-37.200629	4.476122
-1034.742947	-29.689050	4.486118
-1032.940668	-31.952416	4.496115
-1031.003370	-35.195751	4.506112
-1029.637935	-26.389232	4.516109
-1027.503547	-39.290479	4.526106
-1025.161483	-27.927657	4.536102
-1023.411068	-30.632700	4.546099
-1021.643437	-33.787316	4.556096
-1019.818927	-35.315314	4.566093
-1017.897806	-25.929799	4.576090
-1016.114107	-41.119575	4.586086
-1014.230398	-34.696359	4.596083
-1012.400301	-27.457759	4.606080
-1010.261793	-35.185683	4.616077
-1008.490152	-33.160646	4.626074
-1006.673272	-26.494637	4.636070
-1004.757089	-31.264505	4.646067
-1003.157267	-23.595927	4.656064
-1000.981773	-29.820357	4.666061
-999.021235	-27.291862	4.676058
-997.549680	-32.434279	4.686054
-995.213010	-31.554283	4.696051
-993.424956	-35.785779	4.706048
-991.558584	-34.276382	4.716045
-989.835905	-33.261873	4.726042
-988.061792	-35.763847	4.736038
-986.044318	-41.156184	4.746035
-984.057736	-38.712366	4.756032
-982.177378	-37.453082	4.766029
-980.251633	-32.973835	4.776026
-978.519388	-37.681109	4.786022
-976.708485	-43.247235	4.796019
-975.030768	-32.332303	4.806016
-972.822291	-34.134817	4.816013
-971.027998	-37.579436	4.826010
-969.245765	-33.686675	4.836006
-967.073517	-38.980596	4.846003
-965.705561	-39.028766	4.856000
-963.614794	-31.751289	4.865997
-961.472964	-37.152441	4.875994
-959.549219	-29.159860	4.885990
-957.742438	-42.700209	4.895987
-956.174365	-32.358227	4.905984
-954.073177	-34.531970	4.915981
-952.223881	-36.750691	4.925978
-950.519269	-38.032105	4.935974
-948.892053	-31.785700	4.945971
-946.370036	-40.798522	4.955968
-944.775717	-30.975439	4.965965
-942.903232	-35.188822	4.975962
-941.019447	-33.304817	4.985958
-938.959255	-41.285407	4.995955
-937.461466	-36.317712	5.005952
-935.450056	-27.628633	5.015949
-933.197466	-34.220578	5.025946
-931.460945	-29.783659	5.035942
-929.831855	-27.219473	5.045939
-927.754397	-30.584609	5.055936
-926.226731	-32.863982	5.065933
-924.495681	-26.091025	5.075930
-922.247676	-26.657238	5.085926
-920.290435	-30.682061	5.095923
-918.351217	-28.093249	5.105920
-916.610440	-28.572038	5.115917
-914.510047	-24.875359	5.125914
-912.916927	-26.039452	5.135910
-911.089254	-28.739400	5.145907
-908.980977	-24.646100	5.155904
-907.037121	-30.039237	5.165901
-905.338453	-38.465659	5.175898
-903.420164	-23.337214	5.185894
-901.573482	-33.887208	5.195891
-900.051806	-31.488977	5.205888
-897.993620	-34.192614	5.215885
-895.813003	-24.671640	5.225882
-894.052561	-28.848128	5.235878
-892.248680	-29.250150	5.245875
-890.255086	-26.633693	5.255872
-888.162333	-25.335660	5.265869
-886.611931	-32.045813	5.275866
-884.749866	-24.038563	5.285862
-882.661768	-28.971607	5.295859
-881.041718	-27.615361	5.305856
-879.138745	-26.545914	5.315853
-877.282031	-26.127462	5.325850
-875.372989	-25.625799	5.335846
-873.748391	-26.134927	5.345843
-871.396675	-20.143228	5.355840
-869.566174	-32.313701	5.365837
-867.722212	-28.227051	5.375834
-866.053108	-34.994061	5.385830
-864.002831	-29.753078	5.395827
-862.064266	-32.180204	5.405824
-860.053801	-32.428921	5.415821
-858.713694	-27.571743	5.425818
-856.462084	-33.036145	5.435814
-854.651513	-28.108921	5.445811
-852.766178	-26.564549	5.455808
-850.887206	-29.984726	5.465805
-849.078991	-29.910587	5.475802
-847.328248	-29.388332	5.485798
-845.570251	-30.052972	5.495795
-843.308037	-34.137539	5.505792
-841.413109	-27.338610	5.515789
-839.837557	-24.896848	5.525786
-837.614572	-23.101716	5.535782
-835.797186	-26.868864	5.545779
-833.950162	-35.214753	5.555776
-832.161127	-26.464764	5.565773
-830.383881	-27.895067	5.575770
-828.400157	-22.266057	5.585766
-826.444452	-29.075702	5.595763
-824.461878	-22.830743	5.605760
-822.840542	-28.390145	5.615757
-821.116742	-23.119035	5.625754
-818.909871	-24.490118	5.635750
-817.283179	-23.404876	5.645747
-815.541067	-28.669383	5.655744
-813.551678	-30.046747	5.665741
-811.423026	-28.702280	5.675738
-809.394772	-25.372903	5.685734
-807.735418	-27.188537	5.695731
-805.892615	-35.844771	5.705728
-804.014003	-33.996141	5.715725
-802.197585	-29.456633	5.725722
-800.046252	-23.110738	5.735718
-798.413513	-28.375119	5.745715
-796.836134	-35.212683	5.755712
-794.748871	-35.451515	5.765709
-792.775633	-19.188633	5.775706
-791.066978	-20.876353	5.785702
-788.639773	-29.217060	5.795699
-787.061229	-32.748635	5.805696
-785.228031	-28.837031	5.815693
-783.472069	-27.548227	5.825690
-781.523934	-26.719592	5.835686
-779.459792	-24.520085	5.845683
-777.828076	-25.388691	5.855680
-775.942054	-24.363817	5.865677
-774.020680	-29.225914	5.875674
-772.074872	-11.213956	5.885670
-770.131215	-27.763321	5.895667
-768.499789	-19.460167	5.905664
-766.510964	-18.859066	5.915661
-764.674781	-23.903323	5.925658
-762.770698	-18.185736	5.935654
-760.852868	-24.703503	5.945651
-758.836237	-28.183506	5.955648
-757.186820	-22.486790	5.965645
-755.299427	-25.513522	5.975642
-753.267106	-19.649062	5.985638
-751.379514	-24.111025	5.995635
-749.639855	-26.725736	6.005632
-747.731889	-33.878201	6.015629
-745.778323	-29.447404	6.025626
-744.138634	-38.072712	6.035622
-742.024655	-29.824560	6.045619
-740.209663	-27.878871	6.055616
-738.248346	-27.685437	6.065613
-736.636620	-24.339950	6.075610
-734.641970	-24.473932	6.085606
-732.554907	-17.964545	6.095603
-730.885360	-31.250738	6.105600
-728.930999	-25.185912	6.115597
-727.208850	-28.906183	6.125594
-725.359350	-20.273125	6.135590
-722.856875	-27.113233	6.145587
-721.767705	-29.619232	6.155584
-719.592843	-26.292678	6.165581
-717.534810	-32.853341	6.175578
-715.975899	-28.511021	6.185574
-714.254692	-20.760570	6.195571
-711.935713	-30.302805	6.205568
-710.079458	-18.123070	6.215565
-708.366742	-29.158351	6.225562
-706.600920	-21.636067	6.235558
-704.573086	-33.447985	6.245555
-702.885479	-20.991832	6.255552
-700.594906	-33.619384	6.265549
-698.832695	-25.351288	6.275546
-697.225232	-28.227457	6.285542
-695.231513	-28.452832	6.295539
-692.869828	-28.844370	6.305536
-691.557454	-30.601320	6.315533
-689.584228	-24.087915	6.325530
-687.693446	-25.833085	6.335526
-685.968865	-29.943699	6.345523
-684.107332	-32.516262	6.355520
-681.978283	-29.687593	6.365517
-680.226949	-26.545945	6.375514
-678.179600	-31.840186	6.385510
-676.404363	-24.499376	6.395507
-674.584191	-32.641928	6.405504
-672.554576	-29.265279	6.415501
-670.680198	-35.109744	6.425498
-668.878854	-25.602140	6.435494
-667.107770	-32.551104	6.445491
-665.536741	-33.403621	6.455488
-663.335822	-27.750750	6.465485
-661.381901	-21.881574	6.475482
-659.400305	-26.112182	6.485478
-657.782944	-23.669078	6.495475
-655.664350	-27.556852	6.505472
-653.825932	-39.666869	6.515469
-651.994208	-36.703829	6.525466
-650.197355	-21.211533	6.535462
-648.257288	-17.272680	6.545459
-646.377931	-28.895053	6.555456
-644.349146	-22.352589	6.565453
-642.600200	-22.140933	6.575450
-640.831410	-27.505896	6.585446
-639.039040	-23.319237	6.595443
-636.995817	-29.916943	6.605440
-635.230463	-23.842360	6.615437
-633.050087	-27.841033	6.625434
-631.397220	-23.660500	6.635430
-629.525745	-29.078175	6.645427
-627.736266	-22.715347	6.655424
-625.456191	-35.729563	6.665421
-624.094285	-30.771518	6.675418
-622.167512	-24.429043	6.685414
-620.239840	-40.192620	6.695411
-618.230720	-26.455192	6.705408
-616.080152	-32.542684	6.715405
-614.532109	-30.628454	6.725402
-612.559629	-37.063262	6.735398
-611.145809	-27.391069	6.745395
-609.081992	-24.154032	6.755392
-607.162520	-29.639357	6.765389
-605.258029	-28.282572	6.775386
-602.698898	-24.426796	6.785382
-601.248260	-31.236104	6.795379
-599.498876	-23.449012	6.805376
-597.654716	-27.131847	6.815373
-595.695378	-27.935832	6.825370
-593.754646	-31.079903	6.835366
-592.066112	-36.130443	6.845363
-590.387475	-29.822508	6.855360
-588.230640	-27.566588	6.865357
-586.268182	-36.548091	6.875354
-584.784837	-15.566398	6.885350
-582.430094	-19.449207	6.895347
-580.963386	-34.354420	6.905344
-578.920478	-18.266653	6.915341
-576.827545	-30.215191	6.925338
-574.960105	-9.954813	6.935334
-573.216469	-35.725927	6.945331
-571.582345	-44.782852	6.955328
-569.512893	-11.186357	6.965325
-567.472574	-25.150617	6.975322
-565.892265	-32.078510	6.985318
-563.606979	-46.421339	6.995315
-561.887781	-27.591441	7.005312
-560.106000	-55.834821	7.015309
-558.428218	-21.897888	7.025306
-556.639376	-30.180613	7.035302
-554.209832	-25.483064	7.045299
-552.250906	-30.766237	7.055296
-550.996308	-33.327008	7.065293
-548.976929	-20.011126	7.075290
-546.790892	-41.359384	7.085286
-545.102515	-59.914023	7.095283
-543.101249	-31.248540	7.105280
-541.614108	-9.130612	7.115277
-539.262306	-42.836426	7.125274
-537.620887	-24.355640	7.135270
-535.758361	-5.561214	7.145267
-533.687274	-38.405911	7.155264
-532.112384	-31.596644	7.165261
-530.292970	-1.204740	7.175258
-528.095724	-3.565561	7.185254
-526.347690	-31.366232	7.195251
-524.440652	-25.917324	7.205248
-522.257596	-40.892716	7.215245
-520.669469	-25.775896	7.225242
-518.919523	-34.293951	7.235238
-517.134032	-21.974849	7.245235
-514.985830	-31.683838	7.255232
-513.263724	-23.603382	7.265229
-511.049939	-34.668049	7.275226
-509.594898	-30.659506	7.285222
-507.669997	-34.760941	7.295219
-505.608792	-31.141306	7.305216
-503.909054	-22.026259	7.315213
-502.131605	-25.354172	7.325210
-499.766752	-25.108156	7.335206
-498.010752	-33.797684	7.345203
-496.208457	-35.476469	7.355200
-494.334798	-30.181673	7.365197
-492.808039	-21.929479	7.375194
-490.728704	-34.399968	7.385190
-488.740063	-34.265953	7.395187
-486.610823	-36.559030	7.405184
-485.032684	-6.857998	7.415181
-483.160818	-48.788891	7.425178
-481.337385	-11.174213	7.435174
-479.602494	-31.569369	7.445171
-477.529982	-33.376556	7.455168
-475.784297	-35.769413	7.465165
-473.576288	-37.102467	7.475162
-471.956431	-31.184511	7.485158
-470.316663	-33.367825	7.495155
-468.005295	-29.549696	7.505152
-466.183271	-34.769888	7.515149
-464.373263	-32.763188	7.525146
-462.711786	-18.715878	7.535142
-460.603724	-16.425208	7.545139
-458.576046	-29.424248	7.555136
-456.877134	-19.330121	7.565133
-455.098786	-26.704826	7.575130
-453.242331	-14.019640	7.585126
-451.293160	-34.014805	7.595123
-449.516089	-31.990203	7.605120
-447.446080	-19.471747	7.615117
-445.726171	-25.046658	7.625114
-443.599892	-26.666622	7.635110
-441.854651	-24.011692	7.645107
-440.052517	-7.103769	7.655104
-437.908981	-26.155803	7.665101
-436.390224	-26.799305	7.675098
-434.543994	-12.904621	7.685094
-432.293960	-29.071661	7.695091
-430.530271	-23.516099	7.705088
-428.503879	-33.848172	7.715085
-426.761901	-30.835883	7.725082
-425.243146	-26.378002	7.735078
-423.298076	-28.496358	7.745075
-421.158674	-26.164871	7.755072
-419.364658	-33.257851	7.765069
-417.428356	-37.878912	7.775066
-415.755746	-20.173488	7.785062
-413.738518	-33.415552	7.795059
-412.113836	-27.534634	7.805056
-410.024697	-30.831729	7.815053
-407.728461	-33.058250	7.825050
-406.119803	-13.807923	7.835046
-404.227569	-24.852744	7.845043
-402.443384	-26.492254	7.855040
-400.677362	-32.423430	7.865037
-399.004293	-29.780627	7.875034
-397.036555	-39.916999	7.885030
-395.032846	-27.331071	7.895027
-392.845184	-25.127258	7.905024
-391.350235	-32.991908	7.915021
-389.369438	-24.758456	7.925018
-387.534650	-29.249608	7.935014
-385.471647	-29.094224	7.945011
-383.766612	-29.254299	7.955008
-381.703007	-37.269736	7.965005
-379.790638	-32.948881	7.975002
-378.360713	-15.574128	7.984998
-375.959709	-38.456541	7.994995
-374.190937	-25.949917	8.004992
-372.762190	-25.074330	8.014989
-370.680355	-22.460456	8.024986
-368.688404	-23.291569	8.034982
-366.798822	-24.584738	8.044979
-365.073271	-17.467829	8.054976
-363.168800	-28.986661	8.064973
-360.862667	-27.783801	8.074970
-359.091226	-22.679401	8.084966
-357.694732	-26.598469	8.094963
-356.057713	-33.431088	8.104960
-353.461596	-19.218709	8.114957
-351.676870	-29.186895	8.124954
-349.994723	-14.820692	8.134950
-348.082386	-26.890224	8.144947
-345.892448	-33.050089	8.154944
-344.693701	-37.387559	8.164941
-342.674638	-34.567859	8.174938
-340.448074	-33.578056	8.184934
-338.557475	-24.753864	8.194931
-336.800473	-21.818110	8.204928
-335.281605	-28.169242	8.214925
-333.092167	-24.663075	8.224922
-331.137714	-29.078558	8.234918
-329.086510	-32.961611	8.244915
-327.438048	-32.067391	8.254912
-325.429086	-33.142753	8.264909
-323.563054	-17.403836	8.274906
-321.764626	-31.570871	8.284902
-319.747258	-32.991768	8.294899
-318.291335	-22.118239	8.304896
-316.386423	-32.032959	8.314893
-314.358816	-32.904454	8.324890
-312.435485	-28.961066	8.334886
-310.461224	-18.784464	8.344883
-308.741042	-20.772097	8.354880
-306.533504	-26.841587	8.364877
-305.002312	-24.356059	8.374874
-303.040503	-41.724296	8.384870
-301.354213	-11.825628	8.394867
-299.141495	-31.681206	8.404864
-297.257912	-33.371243	8.414861
-295.340423	-26.319658	8.424858
-293.843684	-29.053160	8.434854
-292.029935	-27.803210	8.444851
-289.927826	-35.535788	8.454848
-287.949725	-26.974984	8.464845
-286.197470	-36.641109	8.474842
-284.140304	-21.501069	8.484838
-282.471366	-37.272080	8.494835
-280.275367	-32.533803	8.504832
-278.681315	-41.440484	8.514829
-276.840434	-31.929384	8.524826
-274.770803	-35.447453	8.534822
-273.173467	-30.834651	8.544819
-271.471259	-37.942875	8.554816
-268.992336	-38.542176	8.564813
-267.383627	-41.243008	8.574810
-265.278674	-66.166906	8.584807
-264.071490	-22.065469	8.594803
-261.897579	-15.269508	8.604800
-259.807648	-29.560404	8.614797
-257.866815	-36.184097	8.624794
-256.008859	-27.564615	8.634791
-254.370962	-31.321639	8.644787
-252.237911	-35.951876	8.654784
-250.629448	-28.153060	8.664781
-248.469018	-30.021453	8.674778
-246.679117	-26.010924	8.684775
-245.081281	-25.307505	8.694771
-243.098532	-23.969233	8.704768
-240.871280	-34.904785	8.714765
-239.220101	-26.604376	8.724762
-237.561477	-29.553150	8.734759
-235.764270	-16.758841	8.744755
-233.428765	-29.614230	8.754752
-231.628550	-32.328240	8.764749
-230.068608	-30.350917	8.774746
-228.104602	-19.891560	8.784743
-225.715264	-31.918722	8.794739
-224.284159	-29.665052	8.804736
-222.522984	-34.368539	8.814733
-220.474326	-31.779236	8.824730
-218.425576	-36.639138	8.834727
-216.739506	-26.792234	8.844723
-214.879503	-43.684710	8.854720
-213.037132	-28.912939	8.864717
-210.786513	-38.893808	8.874714
-208.774653	-45.288806	8.884711
-207.408450	-38.880192	8.894707
-205.666480	-34.994610	8.904704
-203.681390	-43.647878	8.914701
-201.635084	-39.495087	8.924698
-199.795809	-34.469284	8.934695
-197.897475	-29.321855	8.944691
-196.204240	-37.285936	8.954688
-194.317978	-27.264129	8.964685
-192.240278	-36.097956	8.974682
-190.453664	-30.833222	8.984679
-188.721465	-40.017681	8.994675
-186.723889	-31.613047	9.004672
-184.372041	-35.990787	9.014669
-183.259541	-39.902329	9.024666
-181.222459	-32.328174	9.034663
-179.317055	-39.934539	9.044659
-177.019696	-51.129102	9.054656
-175.479055	-39.770075	9.064653
-173.625577	-34.838092	9.074650
-171.994122	-33.390018	9.084647
-169.659167	-41.219655	9.094643
-168.003882	-34.078753	9.104640
-166.006704	-31.948539	9.114637
-164.313387	-39.405789	9.124634
-162.210497	-23.090334	9.134631
-160.748252	-36.270499	9.144627
-158.761770	-34.946963	9.154624
-156.600515	-34.514966	9.164621
-154.681160	-43.074029	9.174618
-153.190111	-32.265992	9.184615
-150.866252	-37.499728	9.194611
-149.188897	-45.022311	9.204608
-147.149764	-37.287409	9.214605
-145.644425	-36.952835	9.224602
-143.652366	-36.362780	9.234599
-141.447701	-37.494481	9.244595
-139.955056	-37.465761	9.254592
-138.003511	-31.823108	9.264589
-135.757186	-44.375238	9.274586
-134.258836	-35.706168	9.284583
-132.360476	-38.959957	9.294579
-130.321069	-37.376431	9.304576
-128.615731	-41.475701	9.314573
-126.706220	-44.314438	9.324570
-125.007877	-43.881179	9.334567
-123.045245	-44.874773	9.344563
-121.076736	-32.630322	9.354560
-118.998414	-39.405319	9.364557
-116.988376	-29.834230	9.374554
-115.522000	-39.914090	9.384551
-113.620876	-33.436033	9.394547
-111.752053	-33.224169	9.404544
-109.734506	-34.859651	9.414541
-107.837369	-44.311944	9.424538
-105.985864	-33.695591	9.434535
-104.246157	-36.589321	9.444531
-102.357381	-35.709605	9.454528
-100.482719	-33.048227	9.464525
-98.513443	-33.723927	9.474522
-96.707513	-33.663063	9.484519
-94.910937	-26.759374	9.494515
-92.795892	-34.514388	9.504512
-90.850075	-36.307351	9.514509
-89.214261	-27.606494	9.524506
-87.470355	-27.927292	9.534503
-85.276552	-27.119911	9.544499
-83.569079	-29.874280	9.554496
-81.544842	-26.248364	9.564493
-79.694062	-28.698763	9.574490
-77.934266	-35.710269	9.584487
-76.154015	-31.922270	9.594483
-74.301918	-27.656275	9.604480
-72.252348	-24.122809	9.614477
-70.469316	-26.887646	9.624474
-68.749217	-32.512863	9.634471
-66.525015	-12.193635	9.644467
-64.739837	-25.460022	9.654464
-62.835982	-17.079786	9.664461
-60.987583	-19.204541	9.674458
-59.008840	-24.721023	9.684455
-57.642488	-14.911394	9.694451
-54.869838	-35.509787	9.704448
-53.264701	-42.283451	9.714445
-51.862893	-22.232481	9.724442
-49.843750	-17.508392	9.734439
-47.975580	-27.200763	9.744435
-45.927819	-14.155738	9.754432
-43.999866	-24.672354	9.764429
-42.331337	-15.507741	9.774426
-40.590223	-16.788027	9.784423
-38.498281	-49.624730	9.794419
-36.277854	-20.341521	9.804416
-34.939536	-25.430568	9.814413
-32.760219	-48.013673	9.824410
-31.067396	-11.558637	9.834407
-29.273192	-18.111414	9.844403
-27.305964	-28.793749	9.854400
-24.881284	-59.297798	9.864397
-23.353686	-25.429491	9.874394
-21.696036	-36.237690	9.884391
-20.091162	-22.337289	9.894387
-18.051861	-30.208053	9.904384
-15.867337	-9.882435	9.914381
-13.843456	-20.090663	9.924378
-12.288088	-30.555714	9.934375
-10.616994	-23.432997	9.944371
-8.495408	-34.113097	9.954368
-6.628759	-18.489237	9.964365
-4.847989	-11.551368	9.974362
-3.948760	12.642352	9.984359
-2.437508	58.138903	9.994355
-1.107072	120.812955	10.004352
0.000000	182.248388	10.009357
0.552505	199.581849	10.014362
1.369323	244.748054	10.019367
1.693342	274.474666	10.024371
2.110084	296.256275	10.029376
2.243843	329.540893	10.034381
2.864851	315.505128	10.039386
3.102175	375.960873	10.044391
3.196612	351.010075	10.049395
3.091426	376.932459	10.054400
3.294815	382.036070	10.059405
3.827166	373.475259	10.064410
3.954486	420.201181	10.069415
3.641647	403.619330	10.074419
4.071061	406.209555	10.079424
3.754473	417.399458	10.084429
3.992246	408.451960	10.089434
4.126041	423.275791	10.094439
4.203841	416.170420	10.099443
3.678798	430.250965	10.104448
4.363995	413.468906	10.109453
4.047648	409.564482	10.114458
4.479531	417.006502	10.119463
4.168102	431.423551	10.124467
4.207742	408.501433	10.129472
4.266165	446.708869	10.134477
4.127486	411.698105	10.139482
4.020685	432.704008	10.144487
4.349665	420.562878	10.149491
4.114056	444.052495	10.154496
4.546616	432.061988	10.159501
4.306759	469.351985	10.164506
4.798657	460.726613	10.169511
4.405885	471.980748	10.174515
4.816690	472.090294	10.179520
4.961997	457.201461	10.184525
4.707914	481.681242	10.189530
4.985567	454.039187	10.194535
5.253560	493.806014	10.199539
4.861502	469.612269	10.204544
5.128220	460.992854	10.209549
4.832133	486.524845	10.214554
4.860404	477.147106	10.219559
4.741614	472.135688	10.224563
5.045226	472.661294	10.229568
5.045548	468.811997	10.234573
4.876676	496.728528	10.239578
5.301754	497.304146	10.244583
5.304908	510.027932	10.249587
5.455912	525.779512	10.254592
5.211731	520.527885	10.259597
5.293584	519.556087	10.264602
5.667499	516.653269	10.269607
5.679087	535.006958	10.274611
5.310962	522.413972	10.279616
6.097529	515.280653	10.284621
5.626097	541.392636	10.289626
5.585086	522.851313	10.294631
5.773967	519.260504	10.299635
5.674930	534.637244	10.304640
5.692765	544.753624	10.309645
5.649494	521.045048	10.314650
5.986998	548.767368	10.319655
6.018193	522.686238	10.324659
5.966219	548.983637	10.329664
6.128741	553.422053	10.334669
5.800166	533.674498	10.339674
5.762149	546.187266	10.344679
5.894525	572.983576	10.349683
6.187397	567.695152	10.354688
6.291413	568.733565	10.359693
6.733273	585.616790	10.364698
6.482541	559.605794	10.369703
6.197637	589.051716	10.374707
6.230525	575.133167	10.379712
6.379572	576.670596	10.384717
6.486817	585.090149	10.389722
6.480372	570.630680	10.394727
6.346445	603.278965	10.399731
6.191299	588.305460	10.404736
6.520266	590.919627	10.409741
6.738501	622.627119	10.414746
7.305733	604.193675	10.419751
7.082186	617.991345	10.424755
6.944418	634.367843	10.429760
7.370056	615.696773	10.434765
7.072499	601.720521	10.439770
7.064499	588.388796	10.444775
6.831248	604.618066	10.449779
7.255632	607.483519	10.454784
7.521597	607.376475	10.459789
6.916854	634.192704	10.464794
7.503837	615.289319	10.469799
7.313882	642.007862	10.474803
7.517328	608.988925	10.479808
7.971265	628.445421	10.484813
7.532850	602.066895	10.489818
7.503304	610.334819	10.494823
7.316789	587.659802	10.499827
7.380096	619.697926	10.504832
7.386482	622.615864	10.509837
7.057473	632.975287	10.514842
7.766126	616.272833	10.519847
7.302498	644.052160	10.524851
7.386731	622.292686	10.529856
7.418049	643.890294	10.534861
7.886954	636.984205	10.539866
8.020339	647.528501	10.544871
8.177151	681.486761	10.549875
8.436777	646.804557	10.554880
8.202302	663.655405	10.559885
7.963905	648.404958	10.564890
8.050596	632.741554	10.569895
8.006361	674.310665	10.574899
8.167986	673.975836	10.579904
8.391081	659.052312	10.584909
8.319081	677.643442	10.589914
8.283648	665.377309	10.594919
8.688933	687.369493	10.599923
8.456547	681.418912	10.604928
8.577370	686.450647	10.609933
8.591829	685.727708	10.614938
8.834460	687.841578	10.619943
8.737660	681.416785	10.624947
8.768684	675.231804	10.629952
8.635035	679.228646	10.634957
8.551603	685.685407	10.639962
8.818567	693.887159	10.644967
8.859298	680.358342	10.649971
8.524408	703.305974	10.654976
9.015116	684.234930	10.659981
8.697775	681.819232	10.664986
8.750946	693.625301	10.669991
8.686310	681.422159	10.674995
8.596293	685.583931	10.680000
8.847186	721.817012	10.685005
8.889175	699.018640	10.690010
9.277774	726.659035	10.695015
9.416184	717.317189	10.700019
9.313914	721.633891	10.705024
9.632539	727.657532	10.710029
9.044517	710.715521	10.715034
9.268765	735.773868	10.720039
9.651697	725.364839	10.725043
9.490949	725.008890	10.730048
9.555518	723.227704	10.735053
9.678236	743.798477	10.740058
9.565923	713.012179	10.745063
9.536056	741.403748	10.750067
9.706810	722.330074	10.755072
9.957278	713.801411	10.760077
9.808825	743.908703	10.765082
9.833252	719.491989	10.770087
9.732218	744.026646	10.775091
10.061230	741.676574	10.780096
9.886124	764.302348	10.785101
10.066162	753.253877	10.790106
10.014666	777.597762	10.795111
10.289246	748.490641	10.800115
10.276959	774.791580	10.805120
10.365451	760.083389	10.810125
10.473851	731.165236	10.815130
10.502981	762.215645	10.820135
10.110929	768.671207	10.825139
10.129443	751.985640	10.830144
10.523646	741.685188	10.835149
10.107457	783.484253	10.840154
10.539248	743.232916	10.845159
10.752926	753.628864	10.850163
10.549117	792.741636	10.855168
10.792603	750.610613	10.860173
10.438256	789.529768	10.865178
10.798599	751.984832	10.870183
10.608968	789.251869	10.875187
10.715765	766.446208	10.880192
11.120180	775.039245	10.885197
11.134299	806.743429	10.890202
11.392790	788.516695	10.895207
11.093311	779.892786	10.900211
10.882600	775.458900	10.905216
11.211146	766.455703	10.910221
11.025954	782.269073	10.915226
11.130800	790.648128	10.920231
11.621833	789.510120	10.925235
11.299054	795.323859	10.930240
11.170688	787.629869	10.935245
11.103050	802.065169	10.940250
11.241609	796.183106	10.945255
11.272624	797.376685	10.950259
11.283147	802.616866	10.955264
11.583474	817.961744	10.960269
11.390263	811.558580	10.965274
11.370557	813.509308	10.970279
11.451114	809.596659	10.975283
11.254670	822.819339	10.980288
11.755424	819.227597	10.985293
11.671169	836.746972	10.990298
11.774771	822.465243	10.995303
12.087586	831.164388	11.000307
11.820691	846.807932	11.005312
12.305193	822.431201	11.010317
11.996153	833.199168	11.015322
12.159238	846.615260	11.020327
12.120439	828.399625	11.025331
11.653288	845.538535	11.030336
12.080079	834.963158	11.035341
11.959972	827.026553	11.040346
12.128297	843.550007	11.045351
12.224162	854.491527	11.050355
11.997576	856.926273	11.055360
12.426270	865.559647	11.060365
12.285444	859.559695	11.065370
12.683651	873.886067	11.070375
12.815750	865.521278	11.075379
12.378987	866.070377	11.080384
13.123474	834.391787	11.085389
12.763042	889.886114	11.090394
13.131933	855.354719	11.095399
13.080394	879.761862	11.100403
12.760130	875.621389	11.105408
13.379977	846.239801	11.110413
13.001053	865.928812	11.115418
12.773056	837.360575	11.120423
12.655126	866.627461	11.125427
12.932842	861.007031	11.130432
12.862556	875.770836	11.135437
13.216503	870.018393	11.140442
13.086840	860.605673	11.145447
12.993685	884.245169	11.150451
13.013106	879.686232	11.155456
13.192707	860.716622	11.160461
12.903440	883.251979	11.165466
13.084328	888.105467	11.170471
13.439188	893.245025	11.175475
13.605956	891.264589	11.180480
13.659014	904.472777	11.185485
13.493394	916.399083	11.190490
13.923058	887.978162	11.195495
13.636223	922.782045	11.200499
13.542889	890.235592	11.205504
13.941464	906.463768	11.210509
13.822717	890.328222	11.215514
13.573923	906.770045	11.220519
13.929053	911.501130	11.225523
13.404668	891.386920	11.230528
13.980421	916.544057	11.235533
13.901116	905.697688	11.240538
13.848494	926.836015	11.245543
13.890632	897.677360	11.250547
13.767060	920.763518	11.255552
14.310489	917.574960	11.260557
14.472208	926.929055	11.265562
14.532647	924.044620	11.270567
14.429608	936.885069	11.275571
14.086124	940.920183	11.280576
14.250675	925.117886	11.285581
14.056684	938.300854	11.290586
14.670592	940.018069	11.295591
15.011430	939.407064	11.300595
14.728900	939.455316	11.305600
14.755022	935.791017	11.310605
14.708808	957.038754	11.315610
14.849038	921.629026	11.320615
15.213208	942.125299	11.325619
14.726980	930.467018	11.330624
14.831101	933.810983	11.335629
14.792450	937.463154	11.340634
15.323907	930.329328	11.345639
15.312115	935.014866	11.350643
14.972762	934.015607	11.355648
14.686361	919.064272	11.360653
14.899775	943.372489	11.365658
14.747201	930.621760	11.370663
14.936885	922.151557	11.375667
15.077077	953.077426	11.380672
15.253745	922.599409	11.385677
15.159618	941.572881	11.390682
15.272672	942.430105	11.395687
15.129436	958.487713	11.400691
15.276496	942.186708	11.405696
15.653760	974.757445	11.410701
15.517711	978.697980	11.415706
15.609153	969.342964	11.420711
15.679905	969.243401	11.425715
15.447669	979.002572	11.430720
15.996523	968.833415	11.435725
15.465853	971.729851	11.440730
15.645012	976.753959	11.445735
15.771483	962.192473	11.450739
15.513741	983.593838	11.455744
15.804875	965.016318	11.460749
15.696226	971.625464	11.465754
15.834639	981.927924	11.470759
16.028823	986.280998	11.475763
15.803075	989.890485	11.480768
16.519608	1009.187335	11.485773
16.402596	1010.057605	11.490778
16.692175	1007.340036	11.495783
16.675576	1002.126049	11.500787
16.299854	999.765340	11.505792
16.262957	979.893378	11.510797
16.275989	992.381042	11.515802
16.686685	986.575347	11.520807
16.437067	1011.621444	11.525811
16.457831	1016.074730	11.530816
16.768447	991.302820	11.535821
16.169193	1009.737196	11.540826
16.447171	1009.867936	11.545831
16.988204	1005.418153	11.550835
16.780586	998.739654	11.555840
16.611973	1015.195619	11.560845
16.368387	993.054207	11.565850
16.976625	1016.880094	11.570855
17.034538	1001.869022	11.575859
16.856682	1004.100473	11.580864
17.190297	997.258374	11.585869
17.040324	1005.110483	11.590874
16.996155	1025.713007	11.595879
17.090739	1009.144323	11.600883
17.279901	1057.929866	11.605888
17.530613	1020.822779	11.610893
17.563890	1040.684403	11.615898
16.889149	1005.338229	11.620903
17.441555	1031.527486	11.625907
17.374746	1021.382374	11.630912
17.892092	1054.055529	11.635917
17.249779	1029.714676	11.640922
17.482375	1044.603811	11.645927
17.839198	1027.149589	11.650931
17.483667	1051.879905	11.655936
17.872988	1022.006441	11.660941
17.174492	1052.107487	11.665946
18.212941	1024.297265	11.670951
17.686788	1042.428280	11.675955
17.514753	1034.611810	11.680960
17.534909	1033.850097	11.685965
17.966640	1035.456030	11.690970
17.814035	1032.564553	11.695975
17.672438	1030.179111	11.700979
17.693292	1072.546399	11.705984
18.386236	1057.638990	11.710989
17.851007	1087.065923	11.715994
18.769281	1060.921183	11.720999
18.655282	1052.311681	11.726003
18.590328	1076.177232	11.731008
18.540330	1070.016044	11.736013
18.896492	1040.065829	11.741018
18.854453	1056.213063	11.746023
18.551239	1028.673604	11.751027
18.289923	1046.891695	11.756032
18.887545	1005.808915	11.761037
18.515933	1041.397752	11.766042
18.322615	1013.047568	11.771047
18.467073	1049.790468	11.776051
18.719396	1050.750067	11.781056
19.031055	1061.225228	11.786061
18.803353	1075.151730	11.791066
18.776895	1059.100626	11.796071
18.962545	1066.571221	11.801075
18.923834	1073.994025	11.806080
18.976334	1064.730316	11.811085
19.237865	1059.104507	11.816090
19.295489	1064.170109	11.821095
19.084742	1064.681586	11.826099
19.196481	1057.717149	11.831104
19.309329	1074.847396	11.836109
19.281632	1069.264562	11.841114
19.212002	1060.936568	11.846119
19.032613	1072.849428	11.851123
19.060089	1072.043967	11.856128
19.453736	1065.081871	11.861133
18.922257	1074.090878	11.866138
19.340007	1078.477708	11.871143
19.881889	1081.351327	11.876147
19.469496	1103.854624	11.881152
19.715072	1091.719932	11.886157
19.550769	1105.322528	11.891162
19.848856	1097.088830	11.896167
19.925729	1093.856378	11.901171
19.748411	1103.857615	11.906176
19.879065	1096.465931	11.911181
19.541597	1098.727585	11.916186
19.699105	1092.378745	11.921191
19.995607	1082.864788	11.926195
19.929144	1109.015698	11.931200
20.021322	1104.686366	11.936205
20.090303	1106.047384	11.941210
19.910891	1081.172128	11.946215
20.182530	1117.921723	11.951219
20.166913	1121.038818	11.956224
20.752649	1113.934094	11.961229
20.561068	1127.132619	11.966234
20.618450	1128.885008	11.971239
20.322255	1101.749580	11.976243
20.619492	1114.445914	11.981248
20.852357	1112.980045	11.986253
20.361191	1101.405993	11.991258
20.520355	1114.643182	11.996263
20.662988	1128.378198	12.001267
20.792572	1126.291694	12.006272
20.918919	1122.970917	12.011277
20.835024	1128.891769	12.016282
20.638484	1128.738643	12.021287
20.994509	1108.822756	12.026291
20.942299	1125.651374	12.031296
20.948101	1127.000394	12.036301
20.865363	1110.300601	12.041306
20.894725	1100.501227	12.046311
20.833652	1093.936507	12.051315
20.237321	1106.687049	12.056320
21.035944	1109.656922	12.061325
20.803304	1116.330067	12.066330
20.619151	1096.181803	12.071335
20.594325	1099.749807	12.076339
20.960795	1111.878416	12.081344
21.148647	1114.789587	12.086349
20.834354	1110.163954	12.091354
20.982150	1096.439471	12.096359
20.648924	1094.726421	12.101363
20.627997	1100.977849	12.106368
20.874348	1096.264374	12.111373
21.044958	1101.979037	12.116378
21.104118	1098.582247	12.121383
21.135694	1101.384297	12.126387
20.846240	1084.900437	12.131392
21.181072	1087.277212	12.136397
20.848185	1094.868378	12.141402
21.183101	1079.932894	12.146407
21.135276	1091.345379	12.151411
20.908022	1097.222851	12.156416
21.211816	1092.621643	12.161421
20.996615	1075.326414	12.166426
20.953000	1058.267194	12.171431
21.254116	1061.404722	12.176435
20.979122	1088.063530	12.181440
21.224546	1065.115437	12.186445
20.815038	1063.603796	12.191450
20.437979	1085.344472	12.196455
20.868700	1068.857727	12.201459
20.537388	1055.652836	12.206464
21.120442	1074.706132	12.211469
20.776534	1068.311120	12.216474
20.814194	1064.350050	12.221479
20.995937	1086.335920	12.226483
21.159617	1065.728508	12.231488
20.930243	1071.136363	12.236493
20.774430	1085.376269	12.241498
20.982613	1072.211472	12.246503
20.761105	1065.700740	12.251507
20.790857	1073.721344	12.256512
20.839733	1056.448673	12.261517
20.688278	1077.585636	12.266522
20.749478	1072.326099	12.271527
20.723349	1076.640222	12.276531
20.438357	1085.310292	12.281536
20.705126	1072.979841	12.286541
20.616340	1091.219355	12.291546
20.748730	1071.378614	12.296551
20.821173	1072.404754	12.301555
20.778615	1090.564352	12.306560
21.238430	1068.047271	12.311565
20.751466	1074.652150	12.316570
20.931654	1084.265182	12.321575
21.117997	1074.734107	12.326579
20.431646	1048.358040	12.331584
20.814957	1086.520074	12.336589
20.494206	1063.450972	12.341594
20.627917	1075.976232	12.346599
20.741804	1084.169506	12.351603
20.669916	1066.988627	12.356608
20.725280	1085.299760	12.361613
20.229170	1075.079579	12.366618
20.773950	1090.751620	12.371623
20.697710	1085.074018	12.376627
20.638484	1075.709847	12.381632
20.567912	1078.627536	12.386637
20.825686	1086.062983	12.391642
21.156414	1084.838558	12.396647
21.090158	1068.942028	12.401651
20.883566	1092.610996	12.406656
21.099897	1075.693225	12.411661
21.092148	1082.844584	12.416666
20.925084	1090.809855	12.421671
20.933890	1072.878063	12.426675
20.741624	1088.342802	12.431680
20.989769	1091.957153	12.436685
20.661373	1084.152980	12.441690
20.728056	1091.450170	12.446695
20.891355	1088.602913	12.451699
20.783978	1088.370909	12.456704
20.854415	1087.525478	12.461709
20.946407	1077.342381	12.466714
20.462817	1059.198979	12.471719
20.718799	1075.486361	12.476723
21.015668	1076.465666	12.481728
20.894647	1077.267192	12.486733
20.910071	1077.537585	12.491738
20.573608	1054.953562	12.496743
20.781656	1064.087463	12.501747
20.484055	1074.677160	12.506752
20.902752	1073.952805	12.511757
20.515844	1086.069091	12.516762
20.416251	1104.726672	12.521767
20.811563	1086.655942	12.526771
20.474060	1106.152585	12.531776
20.745269	1067.455651	12.536781
20.878742	1091.388928	12.541786
20.443172	1081.496563	12.546791
20.931285	1093.427554	12.551795
20.745878	1072.724421	12.556800
21.007163	1101.844561	12.561805
20.659877	1072.336072	12.566810
20.938731	1099.384390	12.571815
20.805185	1097.068617	12.576819
20.646932	1096.593985	12.581824
21.073359	1085.386111	12.586829
21.026099	1087.349156	12.591834
20.929184	1098.267992	12.596839
21.170249	1091.743394	12.601843
20.935514	1079.499237	12.606848
21.087555	1094.937450	12.611853
20.806169	1069.911316	12.616858
20.798603	1063.284458	12.621863
21.025858	1066.637200	12.626867
20.978058	1057.145060	12.631872
21.006029	1053.135075	12.636877
20.868591	1043.215684	12.641882
20.628542	1066.025755	12.646887
20.807271	1050.845548	12.651891
20.562685	1048.618459	12.656896
20.551429	1065.992423	12.661901
20.649801	1057.189769	12.666906
20.710290	1045.641314	12.671911
20.681874	1066.924221	12.676915
20.389098	1071.430688	12.681920
21.006651	1075.035000	12.686925
20.786370	1097.351523	12.691930
20.705288	1111.284636	12.696935
21.088206	1094.808640	12.701939
20.919727	1081.596677	12.706944
20.593075	1080.969128	12.711949
20.670125	1076.241662	12.716954
20.988195	1079.466378	12.721959
21.251227	1071.572608	12.726963
20.841222	1074.493973	12.731968
21.177928	1061.758128	12.736973
20.907119	1061.209985	12.741978
20.735680	1070.894864	12.746983
20.975118	1061.926200	12.751987
20.595192	1074.508152	12.756992
20.977815	1068.300039	12.761997
20.742419	1069.331124	12.767002
20.663869	1063.469391	12.772007
20.744280	1074.516047	12.777011
20.588139	1065.930606	12.782016
20.892014	1057.522538	12.787021
20.774652	1074.874012	12.792026
20.957698	1071.564704	12.797031
21.018843	1065.160281	12.802035
20.810334	1074.549869	12.807040
21.200216	1042.613567	12.812045
21.039043	1088.294806	12.817050
20.708412	1064.238503	12.822055
20.771486	1065.956860	12.827059
20.826408	1084.938285	12.832064
20.814304	1079.048600	12.837069
21.146880	1070.115540	12.842074
20.523726	1068.272113	12.847079
20.754053	1080.471298	12.852083
20.886033	1085.801022	12.857088
21.305653	1064.041007	12.862093
20.774269	1079.033111	12.867098
20.839068	1052.363757	12.872103
20.773260	1045.607422	12.877107
20.668738	1041.049280	12.882112
20.681876	1049.693854	12.887117
20.854014	1055.547029	12.892122
20.936556	1059.682961	12.897127
20.981180	1037.806176	12.902131
20.658789	1050.361584	12.907136
20.905848	1044.574082	12.912141
20.517747	1038.857929	12.917146
20.458869	1058.425188	12.922151
20.861731	1060.827379	12.927155
20.711655	1072.511630	12.932160
20.978598	1084.465276	12.937165
20.898070	1091.421661	12.942170
20.773483	1073.077472	12.947175
20.850260	1049.124950	12.952179
20.385730	1070.836978	12.957184
21.077654	1063.634914	12.962189
20.747225	1052.773295	12.967194
20.589687	1088.036356	12.972199
21.016095	1059.673969	12.977203
20.672757	1069.599159	12.982208
20.930289	1082.311260	12.987213
20.957071	1065.373271	12.992218
20.643016	1067.752614	12.997223
20.885021	1068.395308	13.002227
20.828567	1065.879582	13.007232
20.913147	1053.425239	13.012237
20.561383	1058.933038	13.017242
20.292409	1054.380622	13.022247
20.989503	1067.572969	13.027251
20.689856	1083.718744	13.032256
21.015607	1088.806244	13.037261
21.015312	1083.436659	13.042266
20.890951	1070.886314	13.047271
21.126958	1054.842237	13.052275
20.930786	1054.130798	13.057280
21.153675	1044.461447	13.062285
20.663121	1039.323044	13.067290
20.669308	1068.318221	13.072295
20.897016	1050.118147	13.077299
20.951088	1054.430511	13.082304
21.011606	1051.430918	13.087309
20.848858	1052.857278	13.092314
20.595389	1049.358974	13.097319
20.900707	1057.174761	13.102323
20.805442	1060.684603	13.107328
21.046266	1049.615173	13.112333
20.886260	1050.567998	13.117338
20.413583	1052.712437	13.122343
20.518137	1046.816774	13.127347
20.628658	1047.835261	13.132352
20.658577	1055.603510	13.137357
20.713471	1054.987646	13.142362
20.924509	1048.543552	13.147367
20.885449	1057.721594	13.152371
20.628353	1053.582032	13.157376
20.729792	1052.406798	13.162381
20.459744	1049.480432	13.167386
20.309804	1059.731168	13.172391
20.640389	1063.630413	13.177395
20.592320	1084.004979	13.182400
21.204361	1087.370470	13.187405
20.974401	1077.708670	13.192410
20.870133	1061.718860	13.197415
20.951675	1060.004314	13.202419
20.749528	1063.436585	13.207424
20.928934	1061.961901	13.212429
21.026988	1062.231731	13.217434
20.673300	1058.381970	13.222439
20.612045	1055.773969	13.227443
20.487389	1060.856028	13.232448
21.015428	1052.798571	13.237453
20.472407	1067.013485	13.242458
20.670850	1062.468515	13.247463
20.989474	1070.990257	13.252467
20.521526	1078.243402	13.257472
21.064711	1061.965814	13.262477
21.051615	1069.854474	13.267482
20.536884	1075.572781	13.272487
20.813120	1074.674024	13.277491
20.805631	1070.385832	13.282496
21.333017	1067.001101	13.287501
20.985998	1062.864840	13.292506
21.048993	1061.022362	13.297511
20.978945	1060.689784	13.302515
20.688896	1070.884026	13.307520
20.621250	1062.003767	13.312525
21.043555	1065.632911	13.317530
20.586436	1069.979506	13.322535
20.973081	1058.902580	13.327539
20.468339	1077.717791	13.332544
20.775601	1055.584617	13.337549
20.955780	1067.667208	13.342554
20.821683	1064.958857	13.347559
20.735843	1067.689740	13.352563
20.464992	1072.117014	13.357568
20.919431	1070.016551	13.362573
20.989371	1067.469625	13.367578
20.714706	1065.401876	13.372583
20.970077	1064.203665	13.377587
20.612312	1062.849356	13.382592
21.141767	1060.011513	13.387597
20.762068	1072.249643	13.392602
20.800052	1073.934155	13.397607
21.029591	1059.097504	13.402611
20.912917	1074.178001	13.407616
20.837996	1077.548980	13.412621
20.807923	1066.972188	13.417626
20.831397	1062.412548	13.422631
21.139302	1083.493598	13.427635
20.965962	1065.371667	13.432640
20.975799	1054.469966	13.437645
20.966100	1048.619335	13.442650
20.624072	1047.969008	13.447655
20.965794	1022.722140	13.452659
20.442373	1041.606517	13.457664
21.030395	1008.946386	13.462669
20.795454	1052.246991	13.467674
21.058156	1022.758006	13.472679
20.868269	1039.528059	13.477683
20.753667	1041.650076	13.482688
20.804687	1035.857576	13.487693
20.784939	1040.323639	13.492698
20.674631	1029.802251	13.497703
21.148105	1028.320091	13.502707
20.421949	1042.616232	13.507712
20.869315	1032.821195	13.512717
20.698210	1029.726083	13.517722
20.705766	1041.918190	13.522727
20.866318	1019.912551	13.527731
20.404267	1045.233870	13.532736
20.916092	1023.692603	13.537741
20.683986	1032.013577	13.542746
20.363413	1046.724435	13.547751
20.826849	1055.541622	13.552755
20.849882	1060.240570	13.557760
20.997931	1068.224955	13.562765
21.071962	1036.159268	13.567770
20.861232	1047.686014	13.572775
20.985841	1048.227581	13.577779
20.899945	1047.359777	13.582784
20.686088	1025.576280	13.587789
20.601246	1043.977535	13.592794
20.715731	1040.218689	13.597799
20.916066	1053.673188	13.602803
21.001838	1051.688302	13.607808
21.047332	1030.946822	13.612813
20.884924	1033.084348	13.617818
20.856403	1031.204429	13.622823
21.000341	1050.327733	13.627827
21.064254	1033.592021	13.632832
20.970560	1039.631097	13.637837
20.903490	1058.108385	13.642842
20.880877	1052.185694	13.647847
20.963019	1038.515893	13.652851
20.677783	1034.052811	13.657856
21.066409	1039.614401	13.662861
20.664535	1052.311801	13.667866
20.783499	1035.630386	13.672871
20.985586	1046.430527	13.677875
21.113719	1052.678660	13.682880
21.109568	1021.238926	13.687885
20.962165	1008.006321	13.692890
20.609712	1031.742611	13.697895
21.180969	1004.845903	13.702899
20.759949	1013.411468	13.707904
21.015683	1011.664413	13.712909
20.648952	1007.936597	13.717914
20.552952	1012.559897	13.722919
20.492134	1020.337868	13.727923
20.300861	1007.295192	13.732928
20.773916	1015.038470	13.737933
20.595357	1049.011661	13.742938
20.700683	1032.127417	13.747943
21.108153	1038.595923	13.752947
20.941512	1050.828438	13.757952
20.796820	1019.986724	13.762957
20.475932	1021.673276	13.767962
20.529520	1029.174378	13.772967
21.038645	1041.182402	13.777971
20.669067	1044.223471	13.782976
21.027195	1034.624021	13.787981
21.178408	1034.133147	13.792986
20.845565	1023.246703	13.797991
20.907337	1019.573543	13.802995
20.633053	1013.246299	13.808000
20.709189	1012.358961	13.813005
20.535151	1019.844325	13.818010
20.549241	1009.862940	13.823015
20.821713	1017.120961	13.828019
20.724423	1050.701140	13.833024
21.001348	1038.939969	13.838029
20.929560	1036.335228	13.843034
20.932689	1034.369834	13.848039
20.982423	1015.796059	13.853043
20.544447	1024.279177	13.858048
20.752463	1012.593675	13.863053
20.912060	1019.038629	13.868058
20.733307	1009.119543	13.873063
20.677686	1009.022791	13.878067
20.418219	1017.067416	13.883072
21.190104	1021.271585	13.888077
20.827083	1021.742692	13.893082
20.621758	1026.309315	13.898087
20.941720	1024.211384	13.903091
20.671716	1026.127946	13.908096
20.673857	1025.659272	13.913101
20.738159	1026.745056	13.918106
20.855914	1042.579776	13.923111
20.822168	1041.252636	13.928115
20.728414	1038.788596	13.933120
20.902893	1038.640949	13.938125
21.024281	1024.423995	13.943130
20.854536	1025.403603	13.948135
21.309654	1010.002732	13.953139
20.749666	1024.147769	13.958144
20.919272	1017.882188	13.963149
20.807195	1012.495765	13.968154
20.440476	1014.888232	13.973159
20.704709	1023.584205	13.978163
20.243458	1032.965193	13.983168
20.609050	1029.237262	13.988173
20.928329	1044.131495	13.993178
20.658202	1040.096519	13.998183
21.153318	1051.237864	14.003187
20.741396	1049.701378	14.008192
20.952286	1033.954510	14.013210
20.851390	1030.440902	14.018227
20.842034	1016.779658	14.023245
21.103457	1012.775698	14.028263
20.751822	1030.453739	14.033280
20.910762	1027.468101	14.038298
20.680874	1027.183918	14.043315
20.638597	1026.674762	14.048333
20.878315	1024.950342	14.053351
20.620562	1026.484232	14.058368
20.697282	1046.458135	14.063386
21.009715	1064.333879	14.068403
20.914025	1054.156340	14.073421
21.051351	1047.189818	14.078439
21.083257	1055.485313	14.083456
20.886984	1061.811673	14.088474
21.120121	1050.469598	14.093491
21.091189	1056.674886	14.098509
20.960367	1051.980029	14.103527
20.858664	1053.361620	14.108544
21.399174	1048.877424	14.113562
21.232619	1054.248968	14.118579
21.023411	1052.012578	14.123597
21.288778	1051.828719	14.128615
21.073571	1051.337707	14.133632
20.957463	1050.058562	14.138650
21.368706	1050.446017	14.143667
21.167880	1057.547000	14.148685
21.202424	1059.397627	14.153703
21.119930	1064.729026	14.158720
21.084373	1058.935196	14.163738
20.970366	1060.594020	14.168755
20.911544	1056.995047	14.173773
21.560673	1067.907044	14.178791
21.203517	1082.930857	14.183808
21.509761	1088.146779	14.188826
21.563550	1085.324187	14.193843
21.477206	1094.041246	14.198861
21.185616	1092.974125	14.203879
21.418532	1100.331552	14.208896
21.418200	1085.240544	14.213914
21.574222	1092.798989	14.218931
21.353174	1098.707759	14.223949
21.555205	1089.198411	14.228967
21.658092	1084.217736	14.233984
21.324776	1083.932746	14.239002
21.432551	1089.910184	14.244019
21.310458	1095.251056	14.249037
21.602349	1092.832491	14.254055
21.292490	1097.407389	14.259072
21.561685	1095.096259	14.264090
21.557329	1089.775624	14.269107
21.500176	1099.562369	14.274125
21.854951	1104.706065	14.279143
21.617132	1112.763052	14.284160
21.948572	1110.413678	14.289178
22.308055	1120.668795	14.294195
21.682153	1109.480997	14.299213
21.845947	1095.468027	14.304231
21.728366	1106.214491	14.309248
21.759486	1091.215985	14.314266
21.681270	1105.981406	14.319283
21.657254	1123.102379	14.324301
22.129640	1119.001823	14.329319
21.924374	1132.828021	14.334336
21.921843	1135.760487	14.339354
22.225215	1123.293486	14.344371
21.979512	1129.829100	14.349389
22.252507	1126.660087	14.354407
21.886217	1131.033218	14.359424
22.060887	1131.150105	14.364442
22.398570	1124.241249	14.369459
22.177350	1120.613108	14.374477
22.008414	1103.881620	14.379495
21.666027	1116.114230	14.384512
21.771762	1125.182903	14.389530
22.046481	1129.195824	14.394547
22.237822	1138.334219	14.399565
22.126505	1128.569667	14.404583
22.275628	1131.890062	14.409600
22.327742	1123.035368	14.414618
22.221862	1131.969490	14.419635
21.805327	1132.893234	14.424653
22.423988	1120.190335	14.429671
22.286643	1127.825477	14.434688
22.110783	1136.275277	14.439706
22.435188	1126.222584	14.444723
22.334588	1123.482811	14.449741
22.537722	1124.548381	14.454759
22.267253	1130.652231	14.459776
22.228201	1126.480670	14.464794
22.233752	1126.961149	14.469811
22.175748	1133.139647	14.474829
22.683420	1150.259214	14.479847
22.518083	1156.231479	14.484864
22.585827	1142.059184	14.489882
22.767792	1125.004296	14.494899
22.673241	1130.238545	14.499917
22.578024	1125.462482	14.504935
22.416015	1134.962392	14.509952
22.330975	1139.254487	14.514970
22.959567	1137.219497	14.519987
22.683851	1157.394481	14.525005
22.972679	1149.828035	14.530023
23.009321	1137.480642	14.535040
22.758907	1131.562182	14.540058
22.712578	1126.172724	14.545075
22.688924	1131.725991	14.550093
23.005389	1117.789319	14.555111
22.703017	1133.052975	14.560128
22.775142	1134.281011	14.565146
22.742895	1125.919528	14.570163
22.734871	1124.929867	14.575181
22.810087	1123.923783	14.580199
22.830732	1145.610299	14.585216
22.800949	1148.205778	14.590234
23.010310	1164.323767	14.595251
23.035942	1164.986656	14.600269
23.285056	1158.826492	14.605287
23.348034	1144.530690	14.610304
22.858687	1138.236644	14.615322
23.070608	1135.785211	14.620339
22.631765	1141.121568	14.625357
23.243264	1149.071421	14.630375
23.127858	1160.193520	14.635392
22.997784	1164.156187	14.640410
23.096358	1159.591442	14.645427
22.842043	1163.256184	14.650445
23.394869	1168.283372	14.655463
23.105512	1155.254952	14.660480
23.178417	1161.423593	14.665498
23.578394	1159.302373	14.670515
23.271645	1171.401147	14.675533
23.204725	1162.927986	14.680551
23.413100	1149.933437	14.685568
23.312585	1159.307154	14.690586
23.353212	1151.940739	14.695603
23.370668	1155.197201	14.700621
23.576010	1168.835248	14.705639
23.457063	1162.060553	14.710656
23.525234	1163.158665	14.715674
23.587681	1157.014118	14.720691
23.336656	1169.159843	14.725709
23.349165	1159.097102	14.730727
23.716310	1151.628273	14.735744
23.509107	1165.937715	14.740762
23.678090	1166.104273	14.745779
23.376650	1164.038302	14.750797
23.556376	1151.600436	14.755815
23.568773	1153.951669	14.760832
23.311961	1155.276215	14.765850
23.681962	1153.274605	14.770867
23.641218	1165.131963	14.775885
23.644468	1164.201848	14.780903
23.671263	1156.980778	14.785920
23.048191	1169.654593	14.790938
23.493826	1164.466643	14.795955
23.663442	1173.467743	14.800973
23.467441	1161.010363	14.805991
23.289147	1173.145277	14.811008
23.206574	1189.615016	14.816026
23.949511	1183.291136	14.821043
23.579743	1194.151819	14.826061
23.565407	1184.362323	14.831079
23.933515	1193.799739	14.836096
23.888601	1194.835667	14.841114
24.062019	1184.610394	14.846131
23.980303	1198.555371	14.851149
23.926157	1190.316890	14.856167
24.154502	1188.693364	14.861184
24.113253	1191.521908	14.866202
24.254938	1188.974705	14.871219
24.155619	1192.861691	14.876237
24.156813	1186.476798	14.881255
24.459880	1183.051300	14.886272
24.393365	1189.879248	14.891290
24.245200	1190.643789	14.896307
23.941139	1182.751906	14.901325
23.873414	1186.517451	14.906343
24.061674	1190.533168	14.911360
24.107387	1187.705552	14.916378
24.240432	1187.231347	14.921395
24.204973	1193.530540	14.926413
23.972716	1194.377705	14.931431
23.908872	1192.262822	14.936448
24.258112	1203.354886	14.941466
24.519291	1218.096174	14.946483
24.440704	1227.301274	14.951501
24.367168	1217.832649	14.956519
24.322756	1225.453019	14.961536
24.396694	1228.832619	14.966554
24.592768	1222.235733	14.971571
24.225705	1222.873173	14.976589
24.418840	1223.177447	14.981607
24.732064	1212.933001	14.986624
24.627646	1217.199896	14.991642
25.009093	1216.225185	14.996659
24.929339	1224.747793	15.001677
24.935014	1217.695225	15.006695
24.927390	1194.062385	15.011712
24.785516	1191.415696	15.016730
24.889141	1184.095844	15.021747
24.870990	1184.984362	15.026765
24.563036	1197.680296	15.031783
24.568706	1184.513560	15.036800
24.561273	1187.527040	15.041818
24.547880	1178.756690	15.046835
24.355030	1203.149841	15.051853
24.956880	1214.712841	15.056871
25.446982	1214.395610	15.061888
24.998254	1228.575328	15.066906
25.110678	1209.148359	15.071923
24.948454	1199.380868	15.076941
24.815020	1193.741017	15.081959
24.830280	1197.875563	15.086976
24.842514	1210.268761	15.091994
24.880085	1206.309892	15.097011
25.076558	1218.697305	15.102029
25.026701	1214.978889	15.107047
25.122899	1218.913346	15.112064
24.934109	1224.909828	15.117082
25.195912	1219.118840	15.122099
25.253839	1219.823770	15.127117
25.263594	1226.178685	15.132135
25.217016	1212.593977	15.137152
25.196251	1226.011746	15.142170
25.243622	1210.878394	15.147187
25.240792	1222.833569	15.152205
25.111115	1226.192164	15.157223
25.517646	1220.271128	15.162240
25.245805	1219.874084	15.167258
25.410423	1214.414769	15.172275
25.269208	1219.338750	15.177293
25.290833	1217.502806	15.182311
25.314930	1211.921190	15.187328
25.276254	1216.973530	15.192346
25.104528	1220.376582	15.197363
25.299430	1220.454064	15.202381
25.190946	1218.637300	15.207399
25.558985	1207.372685	15.212416
25.389002	1213.032690	15.217434
25.672755	1222.958622	15.222451
25.698484	1219.802288	15.227469
25.659698	1217.673966	15.232487
25.688664	1212.061687	15.237504
25.950648	1214.568170	15.242522
26.037061	1223.534597	15.247539
25.794114	1227.106309	15.252557
25.623616	1215.181989	15.257575
25.705614	1213.696630	15.262592
25.386332	1221.514993	15.267610
25.436152	1217.362262	15.272627
25.668360	1219.683165	15.277645
25.457141	1237.625343	15.282663
25.847438	1246.508709	15.287680
25.926981	1248.742284	15.292698
25.861008	1241.281145	15.297715
26.089811	1242.641498	15.302733
26.519649	1251.609794	15.307751
26.398244	1230.189362	15.312768
25.969537	1221.375120	15.317786
26.484920	1215.815814	15.322803
26.184119	1209.098416	15.327821
25.966591	1210.887024	15.332839
25.717353	1200.729153	15.337856
25.810852	1220.996342	15.342874
26.109531	1225.449050	15.347891
26.249360	1226.941567	15.352909
26.024979	1225.646643	15.357927
26.350512	1246.955927	15.362944
26.206566	1241.324027	15.367962
26.338383	1237.815721	15.372979
26.662142	1236.103040	15.377997
26.318801	1228.948836	15.383015
26.554487	1207.638219	15.388032
26.346682	1217.955575	15.393050
26.099693	1212.959877	15.398067
26.256866	1218.781629	15.403085
26.129561	1229.564340	15.408103
26.438428	1241.844187	15.413120
26.660708	1248.191955	15.418138
26.189094	1240.721585	15.423155
26.440938	1239.004645	15.428173
26.312977	1245.883317	15.433191
26.897872	1237.849616	15.438208
26.588811	1241.195927	15.443226
26.774365	1241.973309	15.448243
26.849045	1241.782110	15.453261
26.478316	1249.188705	15.458279
26.942367	1244.274636	15.463296
26.935763	1236.237754	15.468314
26.868459	1239.363039	15.473331
26.533519	1215.805964	15.478349
26.514548	1228.954470	15.483367
26.984111	1227.932670	15.488384
26.804913	1234.084925	15.493402
26.536271	1231.286992	15.498419
26.794807	1234.122783	15.503437
26.446791	1242.622125	15.508455
26.715191	1231.738317	15.513472
26.852277	1234.939537	15.518490
26.802692	1240.602371	15.523507
26.992624	1245.764545	15.528525
26.814947	1247.162992	15.533543
26.591272	1238.674678	15.538560
26.870136	1243.767612	15.543578
27.042685	1247.109466	15.548595
27.188189	1248.575913	15.553613
26.961102	1261.170917	15.558631
27.209821	1273.985763	15.563648
27.580090	1266.697271	15.568666
27.214712	1245.180454	15.573683
27.253322	1240.872206	15.578701
27.045682	1244.817380	15.583719
27.128637	1246.779857	15.588736
27.303408	1267.568964	15.593754
27.213866	1267.657210	15.598771
27.671237	1269.196610	15.603789
27.802332	1271.681509	15.608807
27.470742	1251.615883	15.613824
27.388015	1243.827087	15.618842
27.381374	1238.294407	15.623859
27.624008	1224.824003	15.628877
27.572974	1238.803450	15.633895
27.528595	1243.924347	15.638912
27.302653	1241.316225	15.643930
27.413269	1244.221228	15.648947
27.771522	1247.794579	15.653965
27.461237	1248.094208	15.658983
27.529235	1260.476982	15.664000
27.699853	1277.763717	15.669018
27.710472	1270.567192	15.674035
27.846578	1266.683824	15.679053
27.711043	1274.016739	15.684071
27.727111	1263.461012	15.689088
27.876535	1257.765010	15.694106
27.759175	1268.168647	15.699123
28.064479	1257.692630	15.704141
27.878117	1248.986004	15.709159
27.832385	1231.668441	15.714176
28.005480	1254.998172	15.719194
27.866567	1250.307686	15.724211
27.932624	1247.266034	15.729229
27.965744	1269.642861	15.734247
27.933328	1265.207512	15.739264
28.040688	1259.579564	15.744282
27.899917	1263.825530	15.749299
28.248575	1262.347970	15.754317
27.777999	1267.989875	15.759335
27.898631	1265.513656	15.764352
27.916376	1284.249912	15.769370
28.044395	1277.928119	15.774387
28.211695	1274.532119	15.779405
28.050207	1273.437940	15.784423
28.258042	1263.721491	15.789440
28.345279	1261.646993	15.794458
28.270747	1268.377158	15.799475
28.469130	1260.738567	15.804493
28.029527	1264.749058	15.809511
27.823688	1265.963239	15.814528
28.523888	1260.766113	15.819546
27.885302	1267.526470	15.824563
28.374917	1266.738992	15.829581
28.336079	1295.296608	15.834599
28.891950	1283.503337	15.839616
28.845716	1291.433912	15.844634
28.260406	1276.237812	15.849651
28.729471	1282.102649	15.854669
28.291317	1282.693229	15.859687
28.845183	1289.853274	15.864704
28.785087	1295.524098	15.869722
28.579854	1297.041772	15.874739
28.905371	1291.449802	15.879757
28.389934	1286.699812	15.884775
28.557412	1286.707739	15.889792
28.542633	1294.729251	15.894810
28.571826	1287.548631	15.899827
28.829095	1283.740313	15.904845
28.714477	1291.213043	15.909863
28.740352	1285.387302	15.914880
28.947973	1289.464451	15.919898
28.803952	1302.307359	15.924915
29.136016	1296.591648	15.929933
28.742908	1292.594485	15.934951
28.813398	1292.632039	15.939968
28.999343	1284.249819	15.944986
28.778164	1291.563371	15.950003
29.243958	1286.469689	15.955021
29.089398	1288.344215	15.960039
29.043089	1285.369240	15.965056
29.137392	1290.954089	15.970074
29.082181	1311.262426	15.975091
29.178254	1309.268308	15.980109
29.175999	1322.801189	15.985127
29.293237	1307.104470	15.990144
29.446334	1316.661203	15.995162
29.304220	1316.817609	16.000179
29.815950	1308.243417	16.005197
29.528965	1298.945634	16.010215
29.500052	1291.651587	16.015232
29.411907	1292.069939	16.020250
29.228080	1286.864371	16.025267
29.292976	1283.133925	16.030285
29.573410	1289.532210	16.035303
29.530304	1303.741684	16.040320
29.761047	1303.396608	16.045338
29.524827	1307.785223	16.050355
29.505873	1306.215285	16.055373
29.457042	1299.715627	16.060391
29.782585	1302.657146	16.065408
29.655371	1305.950873	16.070426
29.736260	1312.270886	16.075443
29.899338	1314.050708	16.080461
29.867748	1319.383520	16.085479
29.880127	1305.845949	16.090496
30.199542	1318.073842	16.095514
29.878031	1310.887801	16.100531
29.916604	1293.169761	16.105549
29.556044	1294.951305	16.110567
29.587527	1303.891937	16.115584
30.002451	1308.538485	16.120602
29.575550	1321.456415	16.125619
30.011389	1312.779497	16.130637
29.975997	1323.871656	16.135655
29.875515	1313.597172	16.140672
30.253021	1313.721035	16.145690
30.164441	1317.246125	16.150707
30.171628	1298.107950	16.155725
30.193869	1303.910360	16.160743
30.284510	1318.718276	16.165760
30.249534	1304.692765	16.170778
29.658009	1314.821286	16.175795
30.250128	1311.782229	16.180813
29.936243	1317.528146	16.185831
30.146394	1310.428763	16.190848
30.630421	1309.550940	16.195866
29.923189	1330.924401	16.200883
30.562739	1334.382123	16.205901
30.472550	1320.755506	16.210919
30.356866	1345.757922	16.215936
30.627280	1335.506062	16.220954
30.591088	1329.444814	16.225971
30.724183	1336.250432	16.230989
30.463813	1341.721986	16.236007
30.457340	1335.932844	16.241024
30.659363	1316.662896	16.246042
30.663400	1337.803374	16.251059
30.603638	1336.845545	16.256077
30.697987	1347.259515	16.261095
30.862550	1333.323271	16.266112
30.919814	1332.587446	16.271130
30.827865	1352.236322	16.276147
31.243889	1322.163478	16.281165
30.717727	1344.668951	16.286183
31.031663	1321.124612	16.291200
30.927823	1333.078687	16.296218
30.917273	1332.243568	16.301235
30.706715	1319.786013	16.306253
31.006731	1338.146987	16.311271
30.454487	1341.401550	16.316288
30.905061	1322.647220	16.321306
30.952629	1332.928644	16.326323
31.167534	1319.852679	16.331341
30.860383	1339.880349	16.336359
30.692829	1325.932591	16.341376
30.990549	1318.388235	16.346394
30.880200	1345.101220	16.351411
31.207512	1351.490482	16.356429
31.323662	1358.259488	16.361447
31.352391	1362.802486	16.366464
31.429966	1349.658737	16.371482
31.607127	1385.200806	16.376499
31.421532	1345.938432	16.381517
31.527222	1350.190730	16.386535
31.059583	1330.549382	16.391552
31.514006	1364.735298	16.396570
31.536644	1351.571996	16.401587
31.302803	1380.511661	16.406605
31.434089	1365.572399	16.411623
31.600742	1354.591472	16.416640
31.521599	1363.408216	16.421658
31.699206	1368.890147	16.426675
31.877644	1353.523385	16.431693
31.771436	1351.921742	16.436711
31.893521	1361.942767	16.441728
32.215910	1364.776266	16.446746
32.162309	1355.705486	16.451763
31.678515	1334.825611	16.456781
31.935324	1342.744058	16.461799
31.836833	1347.816995	16.466816
32.183989	1340.060253	16.471834
31.862745	1344.706255	16.476851
31.486544	1338.343737	16.481869
31.928766	1333.472446	16.486887
31.753596	1354.325358	16.491904
32.308210	1351.803500	16.496922
32.083278	1351.326612	16.501939
32.198787	1360.291629	16.506957
32.162100	1357.429934	16.511975
32.079347	1359.470765	16.516992
32.196236	1360.222926	16.522010
31.892155	1351.108731	16.527027
32.062014	1362.209080	16.532045
32.368127	1352.970819	16.537063
32.067062	1355.202196	16.542080
32.316555	1361.962520	16.547098
32.358328	1368.781145	16.552115
32.204486	1347.523014	16.557133
32.450125	1360.122928	16.562151
32.413939	1358.950555	16.567168
32.281209	1347.333129	16.572186
32.035241	1357.914643	16.577203
32.053258	1365.219967	16.582221
32.315003	1363.210428	16.587239
32.213758	1382.250502	16.592256
32.393617	1378.199680	16.597274
32.564562	1371.738867	16.602291
32.231825	1376.655696	16.607309
32.346551	1375.788010	16.612327
32.417665	1383.452957	16.617344
32.782238	1382.369244	16.622362
32.747750	1390.865854	16.627379
32.900827	1406.580964	16.632397
33.514270	1400.639438	16.637415
33.112427	1392.715845	16.642432
32.747276	1380.625809	16.647450
32.822265	1381.195894	16.652467
32.821155	1373.403448	16.657485
33.026708	1383.072980	16.662503
33.128540	1401.744067	16.667520
33.047139	1384.594029	16.672538
33.006729	1387.370568	16.677555
33.351319	1407.994368	16.682573
33.419651	1391.715480	16.687591
33.085192	1394.340722	16.692608
33.267491	1359.656851	16.697626
33.078660	1384.065394	16.702643
33.262811	1400.450360	16.707661
33.642669	1392.126812	16.712679
33.222394	1392.539939	16.717696
33.379432	1408.375541	16.722714
33.332533	1384.251584	16.727731
33.258992	1423.759953	16.732749
33.713064	1394.821321	16.737767
33.385964	1416.905050	16.742784
33.638477	1412.970043	16.747802
33.950611	1393.391426	16.752819
33.356600	1419.505298	16.757837
33.882268	1400.855292	16.762855
33.437214	1399.630154	16.767872
33.925328	1391.353833	16.772890
33.981038	1405.218888	16.777907
33.665595	1379.029944	16.782925
34.345065	1359.985804	16.787943
33.462748	1376.017031	16.792960
33.933415	1353.770536	16.797978
34.059319	1356.784807	16.802995
33.959420	1361.538654	16.808013
33.482734	1365.386775	16.813031
33.715939	1356.424404	16.818048
33.922009	1375.107146	16.823066
34.159678	1405.909598	16.828083
33.975364	1381.842168	16.833101
33.803121	1406.826970	16.838119
33.372469	1397.250020	16.843136
33.884181	1400.970391	16.848154
33.843491	1380.906951	16.853171
33.987115	1414.620320	16.858189
33.983386	1389.981387	16.863207
33.962217	1407.684254	16.868224
34.073962	1408.887117	16.873242
34.809904	1408.357643	16.878259
34.211058	1418.528300	16.883277
34.682730	1403.333364	16.888295
34.042342	1402.982512	16.893312
34.418277	1400.607121	16.898330
34.511896	1430.498235	16.903347
34.739555	1401.779744	16.908365
34.936697	1426.647463	16.913383
34.703734	1401.598338	16.918400
34.774803	1395.866016	16.923418
34.709509	1415.531175	16.928435
34.111297	1397.804461	16.933453
35.018248	1369.584869	16.938471
34.669607	1416.954920	16.943488
35.210740	1379.780326	16.948506
34.873837	1409.364116	16.953523
34.642377	1379.589478	16.958541
34.693163	1397.243103	16.963559
34.578739	1405.637642	16.968576
34.997497	1409.396437	16.973594
35.002758	1407.869815	16.978611
34.832102	1437.795231	16.983629
35.019887	1426.637848	16.988647
35.083061	1403.481006	16.993664
34.842236	1412.383341	16.998682
34.749802	1431.540050	17.003699
34.926823	1408.530208	17.008717
35.034863	1443.509299	17.013735
35.018380	1411.257423	17.018752
35.318369	1413.757881	17.023770
35.019726	1420.880934	17.028787
35.284678	1398.104046	17.033805
35.333953	1433.963932	17.038823
35.168449	1413.228229	17.043840
35.309347	1402.097220	17.048858
35.513200	1425.367265	17.053875
35.488298	1463.419244	17.058893
35.398775	1440.206475	17.063911
35.939726	1419.229100	17.068928
35.689948	1450.265120	17.073946
35.733585	1421.203138	17.078963
35.654877	1393.846988	17.083981
35.730339	1413.294642	17.088999
35.512347	1426.781807	17.094016
35.487175	1401.572125	17.099034
35.792308	1391.382327	17.104051
35.645186	1448.093876	17.109069
35.953745	1454.753588	17.114087
35.648380	1429.204734	17.119104
35.994915	1408.934777	17.124122
36.235162	1444.408730	17.129139
35.505788	1433.167966	17.134157
36.116803	1412.556948	17.139175
36.041442	1462.167566	17.144192
35.428871	1430.679251	17.149210
35.840496	1435.453781	17.154227
35.821396	1437.777050	17.159245
36.284981	1421.375314	17.164263
35.806975	1461.494130	17.169280
36.018431	1424.269758	17.174298
36.371435	1450.525220	17.179315
36.038573	1443.370810	17.184333
36.605429	1410.085236	17.189351
36.362921	1460.715075	17.194368
36.172752	1465.104257	17.199386
35.979818	1432.051501	17.204403
36.701081	1456.230067	17.209421
36.829483	1488.522462	17.214439
36.409561	1460.223318	17.219456
36.353173	1448.025777	17.224474
36.341426	1444.106169	17.229491
36.537056	1462.696309	17.234509
36.813132	1451.232245	17.239527
36.800153	1462.648121	17.244544
36.856246	1466.139161	17.249562
36.576987	1450.008455	17.254579
36.877544	1481.040135	17.259597
36.408273	1465.065559	17.264615
36.780096	1453.012073	17.269632
36.624290	1472.679162	17.274650
37.269713	1451.370476	17.279667
36.571629	1469.849913	17.284685
36.762858	1443.682285	17.289703
37.007176	1468.092670	17.294720
36.962711	1428.035213	17.299738
37.078852	1467.886252	17.304755
36.861936	1469.943778	17.309773
37.330391	1427.802067	17.314791
36.898574	1478.745305	17.319808
36.746161	1466.331831	17.324826
37.328974	1465.197574	17.329843
37.109053	1513.437735	17.334861
37.276602	1482.745096	17.339879
37.352437	1502.853476	17.344896
37.337138	1478.601627	17.349914
37.716739	1486.602815	17.354931
37.664563	1485.165570	17.359949
37.616429	1494.746652	17.364967
37.681443	1483.497123	17.369984
37.644313	1482.526237	17.375002
37.651332	1488.131376	17.380019
37.662203	1475.654099	17.385037
37.741582	1480.598039	17.390055
37.891011	1438.176848	17.395072
37.521612	1486.377840	17.400090
37.453548	1461.259839	17.405107
37.371968	1479.886349	17.410125
37.524026	1484.908361	17.415143
37.907293	1466.540531	17.420160
37.602695	1487.574725	17.425178
38.101590	1456.865472	17.430195
37.609064	1489.587236	17.435213
37.847914	1457.388914	17.440231
38.031691	1491.494031	17.445248
38.133317	1472.526179	17.450266
37.949918	1492.366008	17.455283
38.032156	1485.631431	17.460301
38.333394	1480.126632	17.465319
38.437048	1486.248036	17.470336
37.870420	1499.004365	17.475354
38.313873	1473.935318	17.480371
38.471724	1527.730933	17.485389
38.716246	1495.512745	17.490407
38.604671	1506.933371	17.495424
38.722877	1468.965564	17.500442
38.669989	1473.504311	17.505459
38.508127	1485.201926	17.510477
38.670628	1479.300833	17.515495
38.551445	1469.188095	17.520512
38.544654	1476.126201	17.525530
38.516136	1469.453342	17.530547
38.537034	1474.845478	17.535565
38.529110	1471.254013	17.540583
38.875227	1481.016022	17.545600
38.830520	1486.627837	17.550618
38.808782	1495.397753	17.555635
38.935434	1498.509461	17.560653
39.066977	1495.435291	17.565671
39.001060	1501.347795	17.570688
38.991317	1509.085480	17.575706
39.362066	1496.222025	17.580723
39.112119	1493.219712	17.585741
39.067743	1479.963162	17.590759
39.059751	1475.251720	17.595776
38.858024	1464.085648	17.600794
38.965659	1493.564102	17.605811
39.068245	1480.488604	17.610829
39.312956	1527.574044	17.615847
39.566921	1485.947719	17.620864
39.374148	1502.847520	17.625882
39.502718	1488.360021	17.630899
39.141643	1525.166469	17.635917
39.281835	1505.314678	17.640935
39.385419	1496.849520	17.645952
39.142595	1509.994658	17.650970
39.752280	1481.628781	17.655987
39.073621	1523.308741	17.661005
39.460673	1501.662093	17.666023
39.666398	1502.516497	17.671040
39.207342	1506.558469	17.676058
39.499545	1501.278471	17.681075
39.428696	1492.622486	17.686093
39.406843	1513.809822	17.691111
40.070728	1517.200789	17.696128
39.901969	1535.671389	17.701146
40.023111	1537.338379	17.706163
39.897960	1531.368313	17.711181
39.917155	1516.075542	17.716199
40.122457	1540.836763	17.721216
40.170600	1539.232503	17.726234
40.381831	1521.949112	17.731251
39.962520	1544.134257	17.736269
40.237417	1530.793705	17.741287
40.477530	1523.626519	17.746304
40.362665	1516.764490	17.751322
40.284246	1528.149957	17.756339
40.320354	1523.964720	17.761357
40.466613	1521.860322	17.766375
40.616807	1515.020512	17.771392
40.333843	1519.183839	17.776410
40.766791	1539.430367	17.781427
40.572182	1511.353162	17.786445
40.623885	1525.171780	17.791463
40.582134	1529.977755	17.796480
40.155694	1509.086906	17.801498
40.657865	1528.528004	17.806515
40.340248	1516.626899	17.811533
40.345353	1549.620212	17.816551
40.520616	1507.245036	17.821568
40.290144	1542.077010	17.826586
40.399494	1524.877506	17.831603
40.548977	1520.337561	17.836621
40.729300	1570.702144	17.841639
41.101238	1540.126222	17.846656
41.140870	1556.317339	17.851674
40.943948	1535.418159	17.856691
40.972294	1555.238458	17.861709
40.661282	1570.061930	17.866727
41.316249	1535.546069	17.871744
41.100039	1578.156015	17.876762
40.797747	1545.482237	17.881779
41.361609	1538.802954	17.886797
40.797890	1560.602170	17.891815
41.676137	1520.842455	17.896832
41.151874	1569.795157	17.901850
41.421265	1543.984543	17.906867
41.457361	1519.002412	17.911885
41.357588	1519.885092	17.916903
41.587697	1567.061079	17.921920
41.387951	1584.725004	17.926938
41.386663	1596.793500	17.931955
41.506712	1585.425002	17.936973
42.212912	1560.228957	17.941991
42.345266	1569.400630	17.947008
41.678534	1568.498695	17.952026
41.954838	1523.644000	17.957043
42.052015	1559.175661	17.962061
41.623790	1544.654215	17.967079
41.995052	1537.146781	17.972096
41.748879	1550.460803	17.977114
42.002291	1539.066352	17.982131
41.794228	1548.514102	17.987149
42.207891	1539.211379	17.992167
42.127864	1573.847975	17.997184
42.200192	1557.642196	18.002202
41.937421	1572.838648	18.007219
42.370033	1550.744214	18.012237
42.395368	1586.148973	18.017255
42.579719	1552.047907	18.022272
42.487785	1559.418056	18.027290
42.318309	1544.685455	18.032307
42.596074	1562.517011	18.037325
42.294082	1537.953711	18.042343
42.366642	1569.152506	18.047360
42.101220	1599.384378	18.052378
42.502857	1556.876997	18.057395
42.483869	1578.620820	18.062413
42.320409	1570.690567	18.067431
42.742125	1554.087720	18.072448
42.467219	1587.668473	18.077466
42.517243	1552.604116	18.082483
42.878673	1580.813738	18.087501
42.469761	1568.862657	18.092519
42.807704	1584.903980	18.097536
42.673336	1579.424575	18.102554
42.871429	1588.176788	18.107571
43.017368	1601.256858	18.112589
42.736258	1600.154990	18.117607
43.140488	1607.598613	18.122624
43.034532	1599.479847	18.127642
42.961676	1617.126719	18.132659
43.331784	1594.230505	18.137677
42.959061	1592.344152	18.142695
43.467481	1607.232023	18.147712
43.265509	1581.734048	18.152730
43.129402	1604.603999	18.157747
43.567497	1587.677605	18.162765
43.418431	1597.120696	18.167783
43.585765	1583.907363	18.172800
43.503560	1583.882755	18.177818
43.206833	1602.768680	18.182835
43.765396	1582.091857	18.187853
43.275242	1601.394022	18.192871
43.491501	1570.377250	18.197888
43.476885	1641.823394	18.202906
43.698279	1639.763626	18.207923
43.707224	1617.960033	18.212941
44.000691	1619.352582	18.217959
44.118907	1632.805191	18.222976
44.214310	1600.006511	18.227994
44.146464	1630.878620	18.233011
44.539450	1599.039220	18.238029
44.288329	1586.779812	18.243047
44.476906	1589.137622	18.248064
44.034089	1563.651350	18.253082
44.141892	1575.738610	18.258099
44.233150	1574.934430	18.263117
43.908283	1567.880928	18.268135
44.085514	1583.754400	18.273152
44.252287	1597.106423	18.278170
44.047284	1594.565681	18.283187
44.347871	1614.559720	18.288205
44.270578	1600.970108	18.293223
44.348787	1623.610852	18.298240
44.494683	1604.920484	18.303258
44.371124	1627.143528	18.308275
44.915066	1589.444132	18.313293
44.268166	1633.168993	18.318311
44.758391	1602.163514	18.323328
44.636142	1628.524987	18.328346
44.658253	1596.568565	18.333363
44.596766	1621.479442	18.338381
45.031876	1598.063193	18.343399
45.274476	1648.367778	18.348416
45.479727	1619.340971	18.353434
45.205466	1598.057631	18.358451
45.454886	1607.416724	18.363469
44.715013	1607.105325	18.368487
44.853937	1625.918651	18.373504
44.630225	1612.537998	18.378522
44.999282	1627.976656	18.383539
44.826875	1634.823275	18.388557
45.192142	1626.616753	18.393575
45.200159	1640.505371	18.398592
45.283153	1632.631731	18.403610
45.146621	1625.530859	18.408627
45.299965	1648.209995	18.413645
45.028724	1634.597802	18.418663
45.270538	1653.031382	18.423680
45.453317	1665.399342	18.428698
45.649635	1665.825818	18.433715
45.658006	1655.912831	18.438733
45.579254	1686.165447	18.443751
46.149632	1667.196512	18.448768
46.065557	1656.533773	18.453786
45.932266	1681.254856	18.458803
46.332311	1647.298492	18.463821
45.738355	1684.266755	18.468839
45.652909	1654.864667	18.473856
45.971423	1664.845136	18.478874
45.702681	1659.687582	18.483891
46.294621	1668.051411	18.488909
46.082802	1650.118038	18.493927
46.049715	1677.305378	18.498944
46.200204	1645.536014	18.503962
46.050030	1672.572133	18.508979
46.279951	1642.904264	18.513997
46.102077	1673.949743	18.519015
46.331494	1640.146452	18.524032
46.113163	1666.366015	18.529050
45.961741	1687.947079	18.534067
46.664708	1672.582839	18.539085
46.646759	1687.853622	18.544103
47.009272	1686.277858	18.549120
46.713586	1686.430444	18.554138
46.764281	1689.535432	18.559155
46.627356	1694.046752	18.564173
47.064474	1679.843336	18.569191
46.741132	1674.142349	18.574208
46.803463	1697.578550	18.579226
46.900100	1671.483801	18.584243
46.608937	1703.967863	18.589261
46.968796	1679.473371	18.594279
46.716778	1696.730487	18.599296
47.355276	1684.763267	18.604314
46.714359	1685.118780	18.609331
47.152745	1695.934312	18.614349
46.780014	1678.124097	18.619367
46.925391	1725.123775	18.624384
47.003063	1709.396752	18.629402
47.392711	1723.035817	18.634419
47.645508	1732.182092	18.639437
47.205947	1722.562299	18.644455
47.578149	1685.490948	18.649472
47.780100	1733.716465	18.654490
47.771639	1715.019114	18.659507
47.829585	1720.608355	18.664525
47.679043	1746.976128	18.669543
47.657425	1753.111333	18.674560
47.773972	1726.239373	18.679578
47.588459	1719.876158	18.684595
48.131977	1695.083357	18.689613
47.985129	1702.382112	18.694631
47.842767	1738.396013	18.699648
47.969778	1691.996287	18.704666
48.143701	1728.810732	18.709683
48.362990	1694.439489	18.714701
48.105510	1735.887713	18.719719
48.035223	1695.759701	18.724736
48.381883	1724.330612	18.729754
48.397110	1702.805891	18.734771
48.121026	1718.561473	18.739789
48.277212	1678.164579	18.744807
48.442933	1716.385022	18.749824
48.160520	1716.014816	18.754842
48.664151	1707.576967	18.759859
48.184134	1724.961717	18.764877
48.582315	1691.390942	18.769895
48.490237	1735.710319	18.774912
48.686694	1704.095519	18.779930
48.530328	1731.938131	18.784947
48.801833	1698.047767	18.789965
48.628779	1746.276507	18.794983
48.769426	1715.954185	18.800000
49.109423	1741.153595	18.805018
48.600606	1728.699210	18.810035
49.127877	1730.979430	18.815053
48.939403	1727.872880	18.820071
49.023666	1719.305280	18.825088
49.106811	1734.471898	18.830106
49.280223	1727.979074	18.835123
49.157905	1717.701493	18.840141
49.064764	1742.814256	18.845159
48.864491	1734.318770	18.850176
49.121126	1725.409066	18.855194
48.730614	1716.163704	18.860211
49.216944	1767.005560	18.865229
49.270509	1765.763783	18.870247
49.492061	1765.926685	18.875264
49.545536	1770.944070	18.880282
49.194009	1736.913881	18.885299
49.740971	1775.488959	18.890317
49.625537	1738.861764	18.895335
49.608754	1763.388224	18.900352
49.607189	1737.914641	18.905370
49.733831	1787.591682	18.910387
50.283469	1760.888114	18.915405
50.229282	1784.531805	18.920423
50.308222	1765.661571	18.925440
49.742540	1741.394815	18.930458
50.055605	1769.442631	18.935475
50.394398	1783.001773	18.940493
50.410967	1748.422058	18.945511
50.007478	1783.323104	18.950528
50.402860	1756.450661	18.955546
50.012991	1789.082791	18.960563
50.171149	1778.763580	18.965581
50.295929	1767.584525	18.970599
50.442982	1793.684693	18.975616
50.813326	1771.686374	18.980634
50.553284	1779.048839	18.985651
51.000163	1774.566778	18.990669
50.590104	1782.683065	18.995687
50.465549	1774.568740	19.000704
50.505924	1773.719181	19.005722
50.681913	1755.977086	19.010739
50.518070	1779.226120	19.015757
50.459162	1780.632415	19.020775
50.153234	1766.902931	19.025792
50.669666	1808.880745	19.030810
50.545767	1785.078292	19.035827
50.660018	1808.223243	19.040845
50.883549	1789.471492	19.045863
50.682289	1820.429776	19.050880
51.203385	1797.790738	19.055898
51.325275	1839.976288	19.060915
51.462609	1833.045571	19.065933
51.704199	1828.569493	19.070951
51.586600	1828.283111	19.075968
51.910223	1815.851617	19.080986
51.394808	1802.355287	19.086003
51.858839	1818.423952	19.091021
52.049622	1808.884469	19.096039
51.601161	1788.234256	19.101056
51.695325	1786.709146	19.106074
51.368687	1792.108065	19.111091
51.472677	1797.735610	19.116109
51.533856	1810.675229	19.121127
51.764365	1819.315446	19.126144
51.967601	1809.275319	19.131162
52.022298	1813.668023	19.136179
52.247828	1805.362564	19.141197
52.438419	1804.685677	19.146215
52.324799	1821.636146	19.151232
52.546268	1819.485104	19.156250
52.316864	1809.809711	19.161267
52.135039	1803.971269	19.166285
52.666009	1805.566636	19.171303
52.661899	1814.563598	19.176320
52.671622	1811.173731	19.181338
52.576553	1802.466367	19.186355
52.554029	1801.401893	19.191373
52.736356	1815.697039	19.196391
52.513463	1801.054494	19.201408
52.649079	1808.975225	19.206426
52.648855	1816.982121	19.211443
52.571855	1799.266164	19.216461
52.630586	1828.161632	19.221479
52.579628	1801.602543	19.226496
52.934437	1821.520580	19.231514
52.933065	1825.145143	19.236531
53.234767	1844.705160	19.241549
53.326543	1830.880724	19.246567
53.066406	1845.726249	19.251584
53.546904	1817.260774	19.256602
53.121055	1834.592968	19.261619
53.356903	1836.373836	19.266637
53.342424	1826.793144	19.271655
53.020353	1844.859145	19.276672
53.320517	1841.035978	19.281690
52.999826	1836.191817	19.286707
53.104710	1838.018741	19.291725
53.569458	1841.988973	19.296743
53.470854	1864.353120	19.301760
53.698558	1819.694031	19.306778
53.913597	1833.411387	19.311795
53.740415	1845.087500	19.316813
53.690066	1815.155662	19.321831
53.753945	1871.764426	19.326848
54.141024	1852.590099	19.331866
53.856850	1879.361678	19.336883
53.890949	1863.529750	19.341901
54.378474	1851.363101	19.346919
53.984023	1857.856693	19.351936
54.317998	1859.138986	19.356954
54.272225	1868.808029	19.361971
54.192650	1868.462097	19.366989
54.203750	1859.313041	19.372007
54.250832	1851.976703	19.377024
54.300365	1861.745374	19.382042
53.948384	1865.120692	19.387059
54.030482	1862.285570	19.392077
54.406940	1869.002289	19.397095
54.216569	1892.026067	19.402112
54.642231	1878.074402	19.407130
54.398787	1898.238972	19.412147
54.386401	1891.610537	19.417165
54.407205	1882.452054	19.422183
54.980582	1914.103409	19.427200
54.968567	1930.180480	19.432218
55.218707	1913.985272	19.437235
55.025911	1906.393002	19.442253
55.444598	1911.585002	19.447271
55.628669	1909.773401	19.452288
55.695539	1884.702360	19.457306
55.818536	1889.703979	19.462323
55.800934	1881.180845	19.467341
55.583964	1874.701453	19.472359
55.801140	1853.345650	19.477376
55.767987	1861.036919	19.482394
55.524674	1878.550843	19.487411
55.400892	1860.686540	19.492429
55.580681	1858.013593	19.497447
55.252765	1856.761863	19.502464
55.362289	1877.277531	19.507482
56.019023	1868.360560	19.512499
55.795685	1887.447511	19.517517
55.997940	1902.170582	19.522535
56.121746	1893.701968	19.527552
56.236344	1880.814534	19.532570
55.890954	1908.484707	19.537587
55.919738	1892.134486	19.542605
56.656014	1888.839514	19.547623
55.981251	1899.994759	19.552640
56.103421	1891.554722	19.557658
55.929091	1879.248210	19.562675
56.265610	1898.727241	19.567693
56.098591	1872.894409	19.572711
56.042565	1905.445241	19.577728
56.202389	1888.938841	19.582746
56.281500	1928.594128	19.587763
56.212019	1930.098080	19.592781
56.754989	1908.638326	19.597799
56.799396	1939.645775	19.602816
56.660277	1931.546269	19.607834
56.595814	1921.772134	19.612851
56.715523	1926.857663	19.617869
57.050315	1934.260621	19.622887
56.960699	1929.532162	19.627904
57.135209	1936.086060	19.632922
57.194003	1959.992023	19.637939
57.038703	1942.118489	19.642957
57.423946	1960.029352	19.647975
57.484294	1953.414458	19.652992
57.199281	1939.808891	19.658010
57.863709	1949.863382	19.663027
57.446723	1946.398388	19.668045
57.638557	1952.422555	19.673063
57.434023	1962.609350	19.678080
57.648516	1945.323365	19.683098
57.829823	1944.029738	19.688115
57.732621	1954.468404	19.693133
57.705690	1955.180612	19.698151
57.930648	1940.408296	19.703168
57.915802	1948.527711	19.708186
57.915895	1942.584691	19.713203
57.679840	1939.300062	19.718221
57.997751	1940.441775	19.723239
57.765306	1946.382592	19.728256
57.901880	1952.859176	19.733274
58.056305	1962.905349	19.738291
58.200353	1976.428092	19.743309
58.503163	1971.061289	19.748327
58.625000	1981.499648	19.753344
58.241429	1976.387034	19.758362
58.579092	1978.220897	19.763379
58.592048	1983.405271	19.768397
58.602586	1970.208730	19.773415
58.727995	1974.009744	19.778432
58.882957	1963.648439	19.783450
59.175046	1986.776324	19.788467
58.761510	1973.178639	19.793485
59.011586	1971.785951	19.798503
58.699411	1990.758214	19.803520
58.696861	1961.877126	19.808538
58.858428	1970.901246	19.813555
58.919354	1981.780340	19.818573
58.715964	1985.331767	19.823591
59.325898	1989.790132	19.828608
58.947507	2020.914737	19.833626
58.827357	1996.316151	19.838643
58.968351	2004.670299	19.843661
58.999119	2009.809369	19.848679
59.314009	1986.142677	19.853696
59.533133	2035.323672	19.858714
60.088861	2010.474118	19.863731
59.901893	2045.476543	19.868749
60.151895	1998.887903	19.873767
59.548975	2024.850901	19.878784
59.781846	2000.543655	19.883802
60.421898	2016.935264	19.888819
60.116932	2011.508072	19.893837
60.068196	1985.250322	19.898855
60.288787	2004.043249	19.903872
60.339575	1976.399498	19.908890
60.150565	2012.045553	19.913907
60.283586	1983.495168	19.918925
60.259101	2009.893652	19.923943
60.205932	1995.250584	19.928960
60.327812	2010.524575	19.933978
60.335470	2029.858811	19.938995
60.290606	2012.429274	19.944013
60.141362	2025.788833	19.949031
60.448539	2000.341843	19.954048
60.127385	2019.440634	19.959066
60.878656	2026.527885	19.964083
60.666820	2036.749717	19.969101
60.709778	2060.158133	19.974119
60.915016	2050.779786	19.979136
60.618393	2042.506344	19.984154
60.890259	2057.091839	19.989171
60.817021	2055.709807	19.994189
61.016793	2039.917334	19.999207
61.376224	2061.441861	20.004224
60.984647	2064.772414	20.009242
61.468629	2062.912963	20.014259
61.424443	2083.644566	20.019277
61.734473	2085.721171	20.024295
61.548234	2095.121747	20.029312
61.569720	2056.764334	20.034330
61.907542	2080.415203	20.039347
61.866605	2068.056581	20.044365
61.652879	2077.466248	20.049383
62.025335	2070.684330	20.054400
61.743729	2077.620146	20.059418
61.998785	2063.793045	20.064435
61.987416	2073.990797	20.069453
62.302946	2079.983491	20.074471
62.319975	2083.895417	20.079488
61.991196	2087.598218	20.084506
62.206112	2056.210952	20.089523
61.845448	2077.607306	20.094541
62.272952	2075.597980	20.099559
62.215286	2062.869212	20.104576
62.062490	2060.786477	20.109594
62.507246	2082.849577	20.114611
62.569413	2074.706878	20.119629
62.655285	2099.228544	20.124647
62.757774	2077.752274	20.129664
62.663610	2095.830216	20.134682
63.207754	2083.653558	20.139699
62.795618	2081.386445	20.144717
62.769914	2097.384871	20.149735
63.018827	2080.621005	20.154752
62.997170	2079.465134	20.159770
62.841322	2096.701879	20.164787
63.003735	2068.934752	20.169805
63.087441	2097.964418	20.174823
63.434751	2077.852291	20.179840
62.997776	2080.152642	20.184858
63.534831	2098.314754	20.189875
63.174359	2092.473224	20.194893
63.126276	2124.007068	20.199911
63.391682	2089.603154	20.204928
63.761057	2119.340809	20.209946
64.026908	2085.488986	20.214963
63.464480	2134.577878	20.219981
63.485179	2109.660896	20.224999
63.672819	2082.862672	20.230016
63.377528	2122.774050	20.235034
63.704744	2140.456855	20.240051
63.909174	2137.208899	20.245069
63.826873	2136.085504	20.250087
63.996459	2148.890154	20.255104
64.201868	2138.034596	20.260122
64.158595	2147.585444	20.265139
64.036950	2142.390097	20.270157
64.683447	2168.644104	20.275175
64.440933	2162.878905	20.280192
64.189328	2174.561496	20.285210
64.614071	2166.950041	20.290227
64.472885	2175.440530	20.295245
65.048707	2143.446509	20.300263
65.344831	2183.752176	20.305280
64.867248	2144.694659	20.310298
65.400947	2175.301307	20.315315
64.963415	2161.289616	20.320333
65.300101	2164.631465	20.325351
65.460819	2161.482500	20.330368
65.613773	2159.074912	20.335386
65.693956	2140.781316	20.340403
65.531334	2157.255480	20.345421
65.663708	2155.411980	20.350439
65.521130	2141.516083	20.355456
65.815022	2154.587214	20.360474
65.551949	2150.574572	20.365491
65.741457	2135.647258	20.370509
65.606706	2153.981079	20.375527
66.279289	2123.577791	20.380544
65.661989	2165.164063	20.385562
65.995686	2126.498687	20.390579
65.814193	2167.889616	20.395597
66.027831	2145.795385	20.400615
65.882665	2146.841863	20.405632
65.459248	2161.654758	20.410650
66.023586	2142.167840	20.415667
65.758465	2137.584498	20.420685
65.903760	2173.726639	20.425703
66.484954	2156.872724	20.430720
66.277937	2178.148763	20.435738
66.394332	2190.719677	20.440755
66.623982	2176.209081	20.445773
66.339935	2184.378639	20.450791
66.541185	2174.931633	20.455808
66.446207	2174.642422	20.460826
66.787579	2174.562843	20.465843
66.588818	2173.531954	20.470861
66.365788	2208.048143	20.475879
67.047680	2188.040600	20.480896
66.731801	2210.146549	20.485914
67.072551	2202.438355	20.490931
66.999359	2205.880977	20.495949
67.268484	2180.550645	20.500967
67.155343	2226.151439	20.505984
67.099183	2219.709168	20.511002
67.694291	2240.568710	20.516019
67.892470	2218.630998	20.521037
67.618860	2262.420910	20.526055
68.540128	2206.735866	20.531072
68.000291	2226.466792	20.536090
67.843311	2220.916027	20.541107
67.773707	2204.225627	20.546125
67.880217	2202.382314	20.551143
68.275980	2205.629018	20.556160
68.055024	2234.550235	20.561178
68.352035	2224.531836	20.566195
67.881760	2233.172375	20.571213
68.291880	2199.969776	20.576231
68.237161	2240.332340	20.581248
67.858105	2238.133861	20.586266
68.536468	2196.540857	20.591283
68.198998	2231.758862	20.596301
68.069126	2231.674211	20.601319
68.273490	2216.289034	20.606336
68.368115	2272.870074	20.611354
68.600993	2265.720984	20.616371
68.389730	2249.335496	20.621389
68.801940	2248.485600	20.626407
69.585306	2225.391924	20.631424
69.025505	2277.814266	20.636442
69.040521	2276.204983	20.641459
69.034398	2252.736141	20.646477
69.105672	2230.797412	20.651495
69.155606	2249.767319	20.656512
69.434039	2269.126333	20.661530
69.366730	2283.249385	20.666547
69.624315	2254.589724	20.671565
69.420495	2296.734946	20.676583
69.626093	2267.234862	20.681600
69.973426	2250.788602	20.686618
69.712468	2283.975460	20.691635
70.000127	2266.088300	20.696653
69.577507	2263.751252	20.701671
70.072265	2265.208512	20.706688
69.520792	2290.314302	20.711706
69.729021	2243.354784	20.716723
69.823515	2296.463327	20.721741
69.554463	2301.497725	20.726759
70.380125	2282.912019	20.731776
70.302335	2295.768049	20.736794
70.410712	2307.021296	20.741811
70.403351	2309.922521	20.746829
70.254832	2292.771887	20.751847
70.516633	2300.593322	20.756864
70.561492	2297.857655	20.761882
70.728063	2326.268130	20.766899
70.682602	2335.456063	20.771917
70.942623	2308.008773	20.776935
71.542472	2315.587531	20.781952
70.980671	2320.814136	20.786970
71.322971	2316.896820	20.791987
71.488612	2313.649506	20.797005
71.654577	2308.685884	20.802023
71.870161	2332.646110	20.807040
71.185689	2314.301203	20.812058
71.721255	2282.107222	20.817075
71.524349	2280.704778	20.822093
71.232544	2337.354776	20.827111
71.425390	2317.382577	20.832128
71.832440	2290.072330	20.837146
71.601708	2331.345727	20.842163
71.849412	2288.269275	20.847181
71.741174	2333.786251	20.852199
72.041194	2317.997154	20.857216
71.761249	2316.258719	20.862234
72.640357	2301.225190	20.867251
72.425286	2333.465700	20.872269
71.757874	2322.336264	20.877287
72.819279	2311.567443	20.882304
72.522004	2349.556638	20.887322
72.528684	2349.554820	20.892339
72.549400	2333.185726	20.897357
72.792336	2335.304532	20.902375
72.559817	2340.090859	20.907392
72.535712	2336.518278	20.912410
72.502021	2324.197610	20.917427
72.562707	2346.474170	20.922445
72.522379	2327.062989	20.927463
72.568053	2350.040408	20.932480
72.887644	2347.467781	20.937498
72.576918	2362.970805	20.942515
73.256176	2364.149314	20.947533
73.114628	2351.127701	20.952551
72.894440	2354.379071	20.957568
73.147071	2382.226129	20.962586
73.311069	2391.268215	20.967603
73.264627	2381.120429	20.972621
73.673035	2400.753062	20.977639
73.866359	2387.409794	20.982656
73.972156	2405.026770	20.987674
74.122680	2368.347706	20.992691
73.834473	2377.896080	20.997709
73.890158	2401.627077	21.002727
74.013971	2376.023835	21.007744
74.067424	2388.440568	21.012762
74.429013	2395.728587	21.017779
74.553857	2375.912665	21.022797
74.454448	2383.554212	21.027815
74.547098	2397.819401	21.032832
74.864231	2391.631357	21.037850
74.610601	2368.383495	21.042867
74.676425	2398.800164	21.047885
75.183383	2391.601011	21.052903
74.448254	2394.865296	21.057920
74.777098	2369.708379	21.062938
74.791815	2418.768320	21.067955
75.001722	2391.325720	21.072973
74.845068	2424.460081	21.077991
75.326462	2397.204635	21.083008
75.106082	2406.864913	21.088026
74.989750	2409.525546	21.093043
75.042712	2406.763396	21.098061
75.428932	2430.627354	21.103079
75.319147	2423.366872	21.108096
75.675929	2420.797740	21.113114
75.478514	2448.325779	21.118131
76.252533	2417.407813	21.123149
75.835483	2424.972616	21.128167
75.693104	2440.152342	21.133184
76.072540	2419.181205	21.138202
75.814925	2439.937915	21.143219
76.162684	2440.016990	21.148237
75.796968	2443.292375	21.153255
76.288061	2422.168139	21.158272
76.605167	2477.266440	21.163290
76.112870	2448.189555	21.168307
76.822527	2431.508333	21.173325
76.293473	2471.594020	21.178343
76.800876	2440.458960	21.183360
76.643598	2454.939467	21.188378
76.990021	2416.627604	21.193395
76.841286	2459.807490	21.198413
76.570350	2443.179600	21.203431
76.809100	2430.829551	21.208448
76.639415	2469.007933	21.213466
76.399621	2445.613800	21.218483
77.331341	2474.616737	21.223501
76.834096	2484.878106	21.228519
77.349674	2468.304090	21.233536
76.873220	2482.582253	21.238554
76.898017	2485.751321	21.243571
77.206315	2483.160022	21.248589
77.166358	2514.626558	21.253607
77.346683	2497.714266	21.258624
77.511769	2516.140733	21.263642
77.573073	2535.035261	21.268659
77.974819	2524.363624	21.273677
78.208610	2524.430987	21.278695
78.419623	2523.490461	21.283712
78.723878	2522.129198	21.288730
78.419085	2540.869746	21.293747
78.751386	2515.388750	21.298765
78.224224	2559.946775	21.303783
78.826359	2538.391717	21.308800
78.599992	2535.066862	21.313818
79.107225	2510.326450	21.318835
78.607271	2539.377714	21.323853
78.886944	2504.223312	21.328871
78.799640	2514.341455	21.333888
78.801780	2535.916589	21.338906
79.194539	2510.695750	21.343923
79.316022	2538.847974	21.348941
78.698377	2533.099190	21.353959
79.323405	2494.008829	21.358976
79.283852	2527.312737	21.363994
78.834492	2527.475676	21.369011
79.411959	2515.129744	21.374029
79.375369	2575.789981	21.379047
79.191423	2548.608112	21.384064
79.719982	2513.605917	21.389082
79.302510	2543.840399	21.394099
79.906134	2571.480824	21.399117
79.375881	2557.023393	21.404135
80.095347	2537.755047	21.409152
80.162999	2555.607179	21.414170
80.032096	2608.510544	21.419187
80.145107	2594.382315	21.424205
80.573720	2558.937383	21.429223
80.368436	2589.805128	21.434240
80.390956	2578.053408	21.439258
80.449086	2553.990987	21.444275
80.812160	2537.009391	21.449293
80.644727	2590.140326	21.454311
80.590581	2595.335620	21.459328
81.443399	2578.581061	21.464346
80.808692	2602.341470	21.469363
81.130657	2568.032023	21.474381
81.135719	2617.026527	21.479399
80.986487	2582.564086	21.484416
81.397907	2616.043259	21.489434
81.680385	2593.794217	21.494451
81.541738	2602.085547	21.499469
81.685654	2604.827415	21.504487
81.609401	2584.723934	21.509504
82.010969	2590.263431	21.514522
82.023195	2605.132362	21.519539
81.945750	2583.159401	21.524557
81.821627	2606.190259	21.529575
81.373531	2590.949642	21.534592
81.866568	2585.284849	21.539610
81.966066	2619.804849	21.544627
81.806403	2588.896202	21.549645
81.868302	2587.295139	21.554663
81.874476	2627.256567	21.559680
82.531877	2615.081075	21.564698
82.245852	2642.119420	21.569715
82.706856	2601.702816	21.574733
82.449701	2630.315963	21.579751
82.610372	2619.921034	21.584768
82.710346	2603.502815	21.589786
82.552837	2639.145378	21.594803
82.609488	2630.798740	21.599821
82.784640	2649.907300	21.604839
83.086993	2641.645750	21.609856
83.340352	2665.973336	21.614874
82.809407	2646.416585	21.619891
82.993737	2619.774431	21.624909
83.447017	2686.603937	21.629927
83.034939	2676.802141	21.634944
82.951738	2674.572927	21.639962
83.531604	2668.420738	21.644979
84.167026	2663.835981	21.649997
84.055740	2706.609473	21.655015
84.354542	2682.909611	21.660032
84.262358	2671.018794	21.665050
84.316452	2676.345517	21.670067
84.142132	2661.514229	21.675085
84.690045	2678.060511	21.680103
84.209545	2700.878558	21.685120
85.012072	2688.088360	21.690138
84.824209	2693.774597	21.695155
85.168695	2676.802883	21.700173
84.750828	2662.289667	21.705191
84.539566	2664.233974	21.710208
84.459838	2671.440704	21.715226
84.689243	2667.147228	21.720243
84.497014	2695.374168	21.725261
85.055554	2668.872822	21.730279
85.023014	2696.448186	21.735296
85.164786	2676.721186	21.740314
85.249554	2722.541315	21.745331
85.711808	2703.518281	21.750349
85.696426	2723.472214	21.755367
85.448980	2716.544235	21.760384
86.117651	2706.918517	21.765402
85.715049	2726.841390	21.770419
85.388934	2708.045544	21.775437
85.756840	2714.384896	21.780455
85.802806	2709.980652	21.785472
86.037095	2717.887718	21.790490
86.010912	2711.335048	21.795507
85.943855	2690.767449	21.800525
85.949987	2734.467757	21.805543
86.053611	2744.369193	21.810560
86.390953	2733.326187	21.815578
86.276630	2740.277325	21.820595
86.386659	2738.025938	21.825613
86.583178	2738.242403	21.830631
86.758215	2757.535182	21.835648
86.995011	2761.646643	21.840666
86.780032	2763.092865	21.845683
86.789590	2774.655627	21.850701
87.512650	2759.802263	21.855719
87.084709	2767.890477	21.860736
87.303972	2763.045627	21.865754
87.147359	2766.701475	21.870771
87.536326	2760.737008	21.875789
87.860627	2775.584661	21.880807
87.721417	2792.067605	21.885824
88.259101	2777.587521	21.890842
88.081609	2783.478222	21.895859
88.187614	2772.627034	21.900877
88.153505	2781.755231	21.905895
87.871642	2787.770339	21.910912
88.452311	2773.083613	21.915930
88.086918	2790.515056	21.920947
88.087392	2792.568769	21.925965
88.444607	2784.495821	21.930983
88.698646	2773.510905	21.936000
88.807021	2795.815943	21.941018
88.560890	2779.536885	21.946035
88.565622	2786.162294	21.951053
89.013329	2775.725412	21.956071
88.894020	2779.203053	21.961088
89.278891	2810.076257	21.966106
88.741021	2831.597935	21.971123
89.111840	2813.939898	21.976141
89.296214	2821.541137	21.981159
89.254753	2817.310478	21.986176
89.678059	2807.098494	21.991194
89.455395	2821.407305	21.996211
89.636535	2803.285558	22.001229
89.772840	2807.773311	22.006247
89.493036	2816.787328	22.011264
90.072765	2846.408764	22.016282
89.848019	2814.872885	22.021299
89.779420	2849.310902	22.026317
89.870845	2817.678187	22.031335
89.769931	2848.405554	22.036352
89.865924	2812.302770	22.041370
89.858149	2879.526040	22.046387
90.134834	2839.134242	22.051405
90.762695	2873.003458	22.056423
90.445856	2846.258327	22.061440
90.876489	2865.374409	22.066458
90.360410	2852.644115	22.071475
91.067971	2889.479443	22.076493
91.324121	2880.203356	22.081511
91.449032	2883.582294	22.086528
91.555486	2861.028979	22.091546
91.399257	2897.169088	22.096563
91.260050	2901.394040	22.101581
91.577443	2864.248992	22.106599
91.384203	2891.542798	22.111616
91.200738	2885.653838	22.116634
91.697891	2859.108451	22.121651
91.285310	2899.025709	22.126669
91.560811	2898.405242	22.131687
91.905016	2884.335041	22.136704
91.929687	2933.023072	22.141722
92.074734	2900.993839	22.146739
92.078659	2917.417129	22.151757
92.162563	2909.431747	22.156775
92.796568	2887.459712	22.161792
92.642481	2915.452098	22.166810
93.059847	2941.207599	22.171827
92.413077	2920.688075	22.176845
93.059241	2910.918723	22.181863
93.051489	2954.834284	22.186880
92.935913	2925.702657	22.191898
92.882060	2920.645670	22.196915
93.188783	2899.672857	22.201933
93.376234	2949.170336	22.206951
92.922641	2940.971750	22.211968
92.831134	2930.494108	22.216986
93.793416	2918.276041	22.222003
93.603767	2937.675198	22.227021
94.071225	2983.085873	22.232039
93.466471	2962.595772	22.237056
94.260300	2933.672281	22.242074
93.889491	2982.559624	22.247091
93.889171	2989.491127	22.252109
94.019969	2949.654809	22.257127
94.082467	2948.380832	22.262144
94.071116	2997.748928	22.267162
94.365256	2986.045594	22.272179
93.983569	2991.391586	22.277197
93.932067	2991.347131	22.282215
94.930397	2990.673531	22.287232
95.132907	3040.632218	22.292250
95.060320	3019.859736	22.297267
94.930383	3021.058017	22.302285
95.395370	2999.170976	22.307303
95.417445	3027.295161	22.312320
95.259983	3008.947917	22.317338
95.575670	3012.375908	22.322355
95.368671	3001.708973	22.327373
95.696670	3025.683879	22.332391
95.593478	3007.183250	22.337408
95.837350	3012.847956	22.342426
95.955137	2981.703874	22.347443
95.519933	3021.578666	22.352461
95.662162	3009.750087	22.357479
95.597763	2977.796562	22.362496
95.700092	3011.722379	22.367514
96.157461	3055.281683	22.372531
95.777645	3018.584090	22.377549
96.742689	3007.115131	22.382567
96.321036	3050.954613	22.387584
96.880183	3028.508191	22.392602
96.886068	3075.038140	22.397619
97.122590	3046.518726	22.402637
97.226328	3080.763049	22.407655
97.039364	3064.236684	22.412672
97.349743	3036.513342	22.417690
97.354456	3065.218514	22.422707
97.007983	3067.421985	22.427725
97.337207	3041.770660	22.432743
96.909519	3075.151873	22.437760
97.211565	3045.354811	22.442778
97.351858	3097.712495	22.447795
97.425633	3070.778804	22.452813
97.933882	3103.407510	22.457831
97.614961	3096.937533	22.462848
97.594550	3086.534180	22.467866
98.362910	3077.861410	22.472883
98.364593	3089.107893	22.477901
98.658707	3122.785498	22.482919
98.602808	3134.300775	22.487936
98.466028	3106.660408	22.492954
99.363461	3077.609203	22.497971
98.961580	3095.153802	22.502989
99.204370	3129.419326	22.508007
99.098506	3114.962092	22.513024
98.953431	3099.888928	22.518042
98.836618	3130.197809	22.523059
98.320829	3105.953839	22.528077
99.337641	3100.603342	22.533095
99.561399	3100.006065	22.538112
99.671000	3143.744588	22.543130
100.092588	3148.437877	22.548147
99.338435	3136.210963	22.553165
100.005379	3107.260957	22.558183
99.763223	3095.950618	22.563200
100.062153	3113.758687	22.568218
100.217871	3150.102172	22.573235
100.042784	3141.299001	22.578253
100.010511	3126.817434	22.583271
100.043196	3141.317095	22.588288
100.671575	3141.401771	22.593306
100.745405	3162.164070	22.598323
100.266646	3152.855554	22.603341
100.724104	3137.504562	22.608359
100.432575	3167.923188	22.613376
100.833168	3137.053822	22.618394
101.030384	3199.949488	22.623411
101.273763	3170.852160	22.628429
101.296995	3195.999997	22.633447
100.981209	3203.143161	22.638464
101.094376	3166.754373	22.643482
101.692498	3184.514816	22.648499
101.151146	3192.860473	22.653517
101.383091	3184.762448	22.658535
101.586111	3186.190035	22.663552
101.391786	3212.657897	22.668570
101.840119	3190.312280	22.673587
101.980733	3243.417705	22.678605
101.977997	3263.810856	22.683623
102.122330	3269.629978	22.688640
102.353263	3247.141957	22.693658
102.193861	3235.395121	22.698675
102.538427	3223.270593	22.703693
103.031534	3242.122350	22.708711
102.841539	3280.402056	22.713728
102.422725	3259.884243	22.718746
102.732915	3252.066319	22.723763
103.313950	3239.376257	22.728781
103.789843	3229.185487	22.733799
103.586278	3243.922722	22.738816
103.487895	3234.050855	22.743834
103.754121	3229.145662	22.748851
103.580426	3240.277854	22.753869
103.879723	3235.494029	22.758887
104.129543	3249.322810	22.763904
103.878683	3279.364693	22.768922
103.927920	3307.990086	22.773939
103.825410	3295.795203	22.778957
104.040459	3288.801849	22.783975
104.127905	3281.587359	22.788992
104.187086	3289.020808	22.794010
104.917383	3280.500300	22.799027
104.539697	3333.639149	22.804045
104.903651	3326.449764	22.809063
104.750430	3312.683447	22.814080
104.892677	3286.141183	22.819098
105.232173	3276.808292	22.824115
105.150949	3309.539330	22.829133
104.927536	3340.870141	22.834151
105.014020	3343.688958	22.839168
104.877159	3346.786453	22.844186
104.987606	3332.899410	22.849203
105.393992	3338.601257	22.854221
106.225882	3329.297578	22.859239
106.396907	3359.612949	22.864256
105.900737	3368.075782	22.869274
105.816879	3360.695065	22.874291
105.807305	3354.695589	22.879309
106.725899	3310.809058	22.884327
106.657880	3370.086889	22.889344
106.102297	3392.612778	22.894362
106.743112	3380.026334	22.899379
106.478763	3380.269109	22.904397
106.727432	3388.499905	22.909415
106.967805	3388.474193	22.914432
106.547108	3390.388275	22.919450
106.930537	3364.726169	22.924467
107.040142	3410.922070	22.929485
107.266049	3393.611317	22.934503
107.059688	3388.074271	22.939520
107.500563	3388.084234	22.944538
107.463844	3415.862208	22.949555
107.541647	3419.586241	22.954573
107.991735	3398.287795	22.959591
108.042451	3441.827362	22.964608
107.820548	3424.308735	22.969626
108.283425	3444.892191	22.974643
108.104068	3424.164478	22.979661
108.404728	3456.535247	22.984679
108.338382	3439.768970	22.989696
108.442102	3418.926115	22.994714
108.803087	3450.555702	22.999731
108.587614	3439.218816	23.004749
108.783191	3458.065597	23.009767
109.086125	3456.366221	23.014784
109.200437	3463.580155	23.019802
109.270062	3474.794075	23.024819
109.273040	3443.650800	23.029837
109.439450	3441.760811	23.034855
109.478214	3486.258937	23.039872
109.181970	3476.014925	23.044890
109.448912	3479.844110	23.049907
110.120747	3471.737136	23.054925
110.116639	3457.455270	23.059943
110.376634	3475.488668	23.064960
110.312465	3516.679067	23.069978
109.932336	3491.415391	23.074995
110.071349	3479.581440	23.080013
110.232292	3483.526642	23.085031
110.852093	3504.034028	23.090048
110.610372	3526.337015	23.095066
110.950020	3503.319178	23.100083
111.122437	3502.131458	23.105101
111.076230	3529.583928	23.110119
110.902020	3490.025257	23.115136
111.278082	3531.899862	23.120154
111.582349	3529.413647	23.125171
111.307184	3515.402281	23.130189
111.791224	3525.990871	23.135207
112.141420	3548.252992	23.140224
112.267642	3509.248123	23.145242
112.560263	3531.760892	23.150259
112.553139	3515.923519	23.155277
112.394374	3499.515662	23.160295
112.355490	3509.745551	23.165312
112.837560	3468.194404	23.170330
112.425468	3508.498684	23.175347
112.203446	3505.850187	23.180365
112.634713	3478.788729	23.185383
112.788694	3525.140745	23.190400
112.305666	3529.581959	23.195418
112.872663	3489.219949	23.200435
112.783504	3547.444658	23.205453
112.837316	3542.193298	23.210471
113.340957	3520.642284	23.215488
113.145205	3565.174115	23.220506
113.290580	3547.382025	23.225523
113.124257	3564.476645	23.230541
113.104916	3570.824638	23.235559
114.211197	3539.131578	23.240576
113.784259	3546.792134	23.245594
113.805484	3608.066508	23.250611
114.099565	3628.373505	23.255629
114.116099	3596.292448	23.260647
114.722282	3574.979082	23.265664
114.668206	3603.325760	23.270682
114.725677	3626.835065	23.275699
114.575560	3614.472876	23.280717
114.665145	3626.080187	23.285735
115.179164	3624.345559	23.290752
114.845794	3640.927282	23.295770
115.072448	3639.658534	23.300787
115.340410	3652.987660	23.305805
115.473171	3651.858956	23.310823
115.745108	3657.942644	23.315840
115.540601	3676.528630	23.320858
116.108780	3685.853973	23.325875
115.824791	3655.791993	23.330893
115.905069	3639.845367	23.335911
116.320408	3625.908641	23.340928
116.234135	3671.184000	23.345946
115.761086	3649.458161	23.350963
116.584633	3672.500051	23.355981
116.327383	3702.388066	23.360999
116.362986	3673.270171	23.366016
116.549431	3650.838970	23.371034
116.868349	3686.206737	23.376051
116.734940	3715.910627	23.381069
116.718092	3684.176097	23.386087
117.183067	3721.232356	23.391104
117.098184	3741.120883	23.396122
117.422841	3716.338334	23.401139
118.050615	3703.991259	23.406157
117.936375	3746.306512	23.411175
118.106283	3762.412443	23.416192
117.884334	3736.359300	23.421210
118.231077	3705.070975	23.426227
118.283165	3751.441529	23.431245
117.970777	3733.770981	23.436263
118.741980	3700.143984	23.441280
118.377898	3737.517345	23.446298
118.300705	3707.772332	23.451315
118.709792	3760.905263	23.456333
118.685867	3741.115936	23.461351
119.155305	3756.720213	23.466368
118.600714	3760.509777	23.471386
119.044111	3722.451997	23.476403
119.305514	3765.335134	23.481421
118.965904	3761.950962	23.486439
120.031957	3736.149463	23.491456
119.335028	3741.184928	23.496474
119.699166	3779.111693	23.501491
120.008803	3791.797916	23.506509
120.046729	3778.764498	23.511527
120.177404	3786.930953	23.516544
119.587465	3797.713814	23.521562
120.057747	3792.440005	23.526579
120.503334	3800.079552	23.531597
120.660512	3828.127883	23.536615
121.184925	3829.059051	23.541632
120.468952	3829.858413	23.546650
121.160126	3808.464293	23.551667
121.189232	3817.370664	23.556685
121.218908	3831.540317	23.561703
121.480523	3839.802344	23.566720
121.422197	3852.531563	23.571738
121.537299	3858.567188	23.576755
122.111371	3852.876410	23.581773
121.587310	3838.570101	23.586791
122.153582	3820.193746	23.591808
122.075764	3809.771500	23.596826
121.968661	3820.438838	23.601843
122.078471	3866.348238	23.606861
122.082813	3862.541836	23.611879
122.204762	3858.202221	23.616896
122.660263	3859.409477	23.621914
123.145114	3841.880698	23.626931
123.235087	3857.809903	23.631949
122.558219	3872.856870	23.636967
123.353044	3858.617128	23.641984
122.982184	3893.988407	23.647002
123.460557	3888.725860	23.652019
123.332907	3919.497498	23.657037
123.468792	3894.044642	23.662055
123.791996	3914.370993	23.667072
123.540834	3890.904766	23.672090
123.590094	3935.440342	23.677107
124.007194	3907.845440	23.682125
123.748891	3949.109703	23.687143
124.224191	3921.552693	23.692160
124.394392	3934.777310	23.697178
124.167400	3955.555665	23.702195
124.823932	3932.767457	23.707213
124.679256	3986.883134	23.712231
124.467280	3965.306347	23.717248
125.090242	3934.570549	23.722266
125.080547	3976.537047	23.727283
125.525123	3975.933633	23.732301
125.424832	3959.123402	23.737319
125.498532	3981.332731	23.742336
125.859007	3988.080526	23.747354
125.967980	3969.099607	23.752371
125.965335	3952.597909	23.757389
125.755614	4001.116838	23.762407
126.115150	3972.529597	23.767424
126.666957	3972.424334	23.772442
126.605072	3997.893912	23.777459
126.895353	4010.526774	23.782477
126.541897	3980.305289	23.787495
126.768595	4026.785747	23.792512
126.474080	4000.381061	23.797530
126.926312	3974.706133	23.802547
127.034529	4024.263940	23.807565
126.666534	4038.124335	23.812583
127.091951	4010.194377	23.817600
127.267951	4048.947926	23.822618
126.824570	4048.372824	23.827635
127.649449	4030.297162	23.832653
127.921054	4039.372674	23.837671
127.976326	4069.900704	23.842688
128.340098	4056.959823	23.847706
128.413044	4079.089182	23.852723
128.977425	4069.749826	23.857741
128.896567	4095.783478	23.862759
128.531540	4079.409434	23.867776
128.965697	4048.048229	23.872794
128.709606	4039.386440	23.877811
129.135442	4059.844518	23.882829
128.974324	4107.009308	23.887847
129.237643	4111.489011	23.892864
129.369781	4099.073538	23.897882
129.428889	4074.778759	23.902899
129.521673	4124.441629	23.907917
129.702233	4114.630886	23.912935
130.249600	4095.542926	23.917952
130.090091	4142.719375	23.922970
130.131600	4108.330688	23.927987
130.389132	4133.835314	23.933005
130.198840	4113.696780	23.938023
130.766108	4106.121394	23.943040
130.783359	4130.542567	23.948058
131.001126	4102.344259	23.953075
130.882565	4145.066476	23.958093
130.887093	4153.231225	23.963111
131.381228	4120.455343	23.968128
131.174219	4172.205961	23.973146
130.962664	4156.099993	23.978163
131.714275	4135.118984	23.983181
131.601209	4182.992995	23.988199
131.506270	4187.473210	23.993216
131.711962	4164.094173	23.998234
131.492230	4202.037259	24.003251
132.140738	4162.052947	24.008269
132.180915	4217.908393	24.013287
132.248840	4215.790934	24.018304
132.636268	4209.911881	24.023322
132.949233	4196.773662	24.028339
133.006531	4219.336028	24.033357
132.899579	4197.902629	24.038375
132.896462	4199.271151	24.043392
133.549871	4192.308949	24.048410
133.361197	4248.133349	24.053427
133.530352	4226.201194	24.058445
133.659002	4210.499539	24.063463
134.045294	4203.897733	24.068480
133.949156	4240.826094	24.073498
133.804794	4258.920219	24.078515
134.391771	4238.660720	24.083533
134.527262	4265.286353	24.088551
134.220794	4260.639698	24.093568
134.320751	4243.075059	24.098586
134.707922	4263.327190	24.103603
134.927900	4266.098154	24.108621
134.967037	4258.587239	24.113639
135.362724	4296.574035	24.118656
135.468921	4265.879042	24.123674
135.570095	4262.401651	24.128691
135.688881	4275.127382	24.133709
135.789514	4266.343284	24.138727
135.576070	4255.538792	24.143744
135.847773	4286.548022	24.148762
135.788290	4269.161387	24.153779
136.125974	4311.709859	24.158797
136.380010	4300.868552	24.163815
136.674059	4306.602071	24.168832
136.209549	4307.357420	24.173850
136.424166	4307.227260	24.178867
136.872079	4321.233150	24.183885
137.127199	4319.779663	24.188903
136.773078	4321.155392	24.193920
137.449168	4293.335965	24.198938
137.575339	4353.694425	24.203955
137.547692	4348.115929	24.208973
137.966027	4316.262652	24.213991
138.186994	4342.052736	24.219008
138.312801	4364.976493	24.224026
138.615995	4337.252630	24.229043
138.779950	4342.815749	24.234061
138.900259	4315.250889	24.239079
138.676160	4327.933793	24.244096
138.417544	4302.236338	24.249114
138.874687	4315.748303	24.254131
138.842165	4305.300389	24.259149
138.746604	4343.800663	24.264167
138.869548	4325.722503	24.269184
139.356292	4310.317638	24.274202
139.043797	4360.125384	24.279219
139.341438	4343.268566	24.284237
139.517663	4351.074077	24.289255
139.485626	4375.427211	24.294272
139.474593	4361.829964	24.299290
140.020060	4355.487483	24.304307
139.832258	4407.528506	24.309325
139.733742	4392.911503	24.314343
139.978588	4378.848641	24.319360
140.134058	4420.553288	24.324378
139.922516	4433.812480	24.329395
140.614805	4412.111300	24.334413
140.908671	4457.348924	24.339431
141.144407	4469.347387	24.344448
141.177561	4443.943001	24.349466
141.425535	4448.428403	24.354483
141.453178	4493.872216	24.359501
141.498411	4473.450191	24.364519
141.794583	4478.434532	24.369536
141.699990	4499.536318	24.374554
142.061089	4480.898431	24.379571
142.406755	4485.645962	24.384589
142.389226	4530.907505	24.389607
142.202743	4514.771970	24.394624
142.849051	4503.934832	24.399642
142.642133	4538.368194	24.404659
143.112156	4531.162103	24.409677
142.940281	4544.361576	24.414695
143.029642	4536.733163	24.419712
143.277406	4545.217282	24.424730
143.399643	4552.726280	24.429747
143.646758	4580.577630	24.434765
143.923916	4559.234283	24.439783
144.389874	4544.714350	24.444800
144.661664	4592.779279	24.449818
144.410304	4567.096722	24.454835
144.934126	4599.708203	24.459853
144.801612	4585.127109	24.464871
144.695688	4581.726719	24.469888
144.770608	4577.599715	24.474906
144.955012	4574.248221	24.479923
144.817976	4583.676367	24.484941
145.071892	4611.030299	24.489959
145.616619	4629.127498	24.494976
145.823682	4595.125066	24.499994
145.618277	4617.455383	24.505011
145.813168	4616.599118	24.510029
145.791969	4598.796129	24.515047
145.679219	4637.600423	24.520064
146.142862	4605.764471	24.525082
146.136817	4645.881254	24.530099
146.179939	4620.080848	24.535117
146.213607	4657.624406	24.540135
146.494232	4643.290477	24.545152
146.664829	4668.216740	24.550170
146.821761	4635.417174	24.555187
146.886465	4709.268187	24.560205
147.004712	4701.994596	24.565223
147.173432	4690.550636	24.570240
147.824414	4713.110353	24.575258
147.703385	4728.916812	24.580275
148.027728	4698.592848	24.585293
148.277245	4744.879208	24.590311
148.471667	4711.651832	24.595328
148.417509	4688.638295	24.600346
148.388643	4714.312320	24.605363
148.704971	4754.959356	24.610381
148.593118	4731.125788	24.615399
149.121632	4721.115198	24.620416
149.198231	4759.790500	24.625434
149.403885	4725.478038	24.630451
149.278546	4738.009452	24.635469
149.474641	4768.426799	24.640487
149.390663	4763.632796	24.645504
150.040236	4763.834490	24.650522
149.849928	4775.536116	24.655539
150.053523	4765.178455	24.660557
150.169691	4788.020235	24.665575
149.963922	4818.245302	24.670592
150.172367	4802.991290	24.675610
150.726075	4814.866962	24.680627
150.674160	4855.856200	24.685645
150.654509	4838.157305	24.690663
150.910167	4834.703923	24.695680
151.327377	4843.836962	24.700698
151.355924	4887.916945	24.705715
151.139475	4849.760073	24.710733
152.014531	4862.511265	24.715751
151.681210	4876.429063	24.720768
152.030874	4881.286224	24.725786
152.128225	4890.973775	24.730803
152.200539	4884.671901	24.735821
152.674425	4881.470068	24.740839
152.603261	4933.240250	24.745856
152.806710	4919.434429	24.750874
153.148801	4902.681597	24.755891
153.188913	4941.496145	24.760909
153.695957	4911.344006	24.765927
153.692632	4946.116390	24.770944
153.985691	4917.869902	24.775962
154.071761	4925.042647	24.780979
154.270786	4940.002955	24.785997
154.437250	4908.705418	24.791015
154.290137	4916.228442	24.796032
154.556347	4943.369414	24.801050
154.056153	4929.463371	24.806067
154.344324	4924.554909	24.811085
155.244735	4913.630545	24.816103
154.616118	4954.586926	24.821120
154.762083	4978.859968	24.826138
155.005086	4967.632878	24.831155
155.602696	4947.338462	24.836173
155.552018	4993.805636	24.841191
155.746905	4969.693057	24.846208
155.702099	4988.879084	24.851226
155.597350	4989.813107	24.856243
155.946298	4989.643431	24.861261
156.079712	4993.717733	24.866279
155.852528	5012.257098	24.871296
156.098485	5014.939887	24.876314
156.070966	5027.541699	24.881331
156.681629	5059.787130	24.886349
156.932553	5050.044003	24.891367
157.256738	5060.436570	24.896384
157.096491	5058.440336	24.901402
157.535874	5068.325214	24.906419
157.812971	5107.170068	24.911437
157.942460	5079.200310	24.916455
158.521558	5058.787542	24.921472
158.676967	5089.593590	24.926490
158.446750	5109.043773	24.931507
158.632854	5072.507254	24.936525
159.088311	5085.007720	24.941543
159.328697	5102.268993	24.946560
159.553733	5088.861577	24.951578
159.211339	5117.721301	24.956595
159.555251	5115.392929	24.961613
159.451299	5095.505185	24.966631
159.184223	5121.776460	24.971648
159.509043	5118.960228	24.976666
159.669773	5126.999128	24.981683
159.729433	5132.523322	24.986701
160.098328	5131.562975	24.991719
160.090957	5161.436137	24.996736
160.127635	5153.984160	25.001754
160.473445	5174.520282	25.006771
160.378647	5164.048645	25.011789
160.973761	5196.598165	25.016807
160.951213	5194.314050	25.021824
160.987798	5195.581142	25.026842
161.210523	5211.417486	25.031859
161.478633	5235.703732	25.036877
162.148951	5225.401927	25.041895
161.859206	5236.987606	25.046912
162.292269	5241.764720	25.051930
162.345857	5251.588508	25.056947
162.160131	5279.607749	25.061965
162.775862	5256.419644	25.066983
162.572240	5262.528696	25.072000
162.720314	5260.334586	25.077018
162.957649	5272.423925	25.082035
162.961006	5286.042973	25.087053
163.206924	5279.000489	25.092071
163.115160	5287.215050	25.097088
163.583901	5295.545579	25.102106
163.557015	5305.962041	25.107123
163.544115	5312.347521	25.112141
163.898822	5324.320636	25.117159
163.995753	5327.305742	25.122176
164.109926	5331.129884	25.127194
164.207190	5349.543989	25.132211
164.454144	5378.930186	25.137229
164.800082	5351.491050	25.142247
164.849416	5389.823053	25.147264
165.163391	5392.428984	25.152282
165.712098	5389.920801	25.157299
165.335461	5388.521526	25.162317
165.885114	5422.576705	25.167335
166.045649	5414.989987	25.172352
166.364338	5428.842108	25.177370
166.658412	5405.226732	25.182387
166.596460	5420.972589	25.187405
166.761836	5419.534881	25.192423
167.186282	5432.489805	25.197440
167.104240	5425.970001	25.202458
167.375125	5453.425070	25.207475
167.351489	5446.659929	25.212493
167.774206	5426.693271	25.217511
167.658471	5450.387309	25.222528
167.604924	5435.011567	25.227546
167.857727	5433.483607	25.232563
168.203697	5482.001420	25.237581
168.385613	5454.279850	25.242599
168.196648	5463.907223	25.247616
168.547393	5497.838521	25.252634
169.075725	5472.292044	25.257651
168.712759	5508.997856	25.262669
169.078281	5507.058554	25.267687
169.107498	5486.399302	25.272704
169.039902	5546.239696	25.277722
169.274471	5519.638560	25.282739
169.558524	5547.986211	25.287757
169.776734	5582.944272	25.292775
169.906264	5551.251605	25.297792
170.264408	5559.271067	25.302810
170.643261	5581.265014	25.307827
170.543626	5580.560291	25.312845
170.561271	5584.789320	25.317863
170.766180	5608.034402	25.322880
170.888052	5605.106468	25.327898
171.330575	5612.756905	25.332915
171.086323	5621.571063	25.337933
171.628657	5616.499122	25.342951
171.715803	5647.801847	25.347968
171.945853	5648.892587	25.352986
172.342028	5631.164990	25.358003
171.929952	5671.176220	25.363021
172.467425	5644.057674	25.368039
172.199052	5657.546521	25.373056
172.595745	5691.743149	25.378074
172.877518	5667.173435	25.383091
172.526644	5699.026800	25.388109
173.235217	5699.489748	25.393127
173.526431	5703.518633	25.398144
173.550697	5707.522422	25.403162
174.267471	5712.728859	25.408179
173.832383	5723.858182	25.413197
173.999234	5710.394969	25.418215
174.167239	5731.953865	25.423232
174.541091	5727.223444	25.428250
174.614567	5733.888001	25.433267
174.489291	5758.546231	25.438285
175.020071	5747.712454	25.443303
175.216419	5760.651325	25.448320
175.094722	5761.499983	25.453338
175.857559	5765.569341	25.458355
175.770073	5780.772870	25.463373
175.893560	5770.502021	25.468391
175.794120	5785.430529	25.473408
176.041876	5800.154215	25.478426
176.298043	5804.587593	25.483443
176.433570	5806.717751	25.488461
176.858831	5822.166069	25.493479
176.892262	5826.992933	25.498496
177.252119	5833.672454	25.503514
177.571782	5826.481061	25.508531
177.348727	5855.869981	25.513549
177.403619	5860.051452	25.518567
177.653297	5865.738377	25.523584
177.898966	5872.599764	25.528602
177.989749	5880.011394	25.533619
178.320145	5889.657727	25.538637
178.450046	5874.574057	25.543655
178.863808	5908.680352	25.548672
178.768844	5919.275677	25.553690
179.098965	5919.533842	25.558707
179.253174	5911.750407	25.563725
179.675315	5919.682763	25.568743
179.719619	5941.132661	25.573760
179.428762	5929.830251	25.578778
179.920921	5946.898959	25.583795
179.902448	5940.886471	25.588813
180.562462	5975.760862	25.593831
180.630714	5957.250420	25.598848
180.697904	5975.897472	25.603866
180.667609	5965.732827	25.608883
180.934118	5981.477264	25.613901
180.830000	5994.907973	25.618919
181.329388	5974.065292	25.623936
181.153519	5998.144287	25.628954
181.583128	6002.124441	25.633971
181.329794	6009.962346	25.638989
181.714895	6032.346987	25.644007
182.168677	6036.479860	25.649024
182.325825	6054.893165	25.654042
182.522153	6049.493098	25.659059
182.644950	6064.793206	25.664077
182.716290	6071.025541	25.669095
182.928772	6075.472261	25.674112
182.909447	6092.816228	25.679130
183.339842	6090.711520	25.684148
183.315479	6107.106695	25.689165
183.655885	6110.187677	25.694183
183.742551	6126.296887	25.699200
184.003007	6143.866952	25.704218
184.440439	6142.139546	25.709236
184.518495	6155.358827	25.714253
184.504398	6134.135177	25.719271
185.056247	6168.668509	25.724288
185.334391	6150.862340	25.729306
185.248435	6180.900363	25.734324
185.264758	6169.974430	25.739341
185.673711	6195.466361	25.744359
186.096497	6187.742240	25.749376
185.647207	6190.909806	25.754394
186.129546	6200.829515	25.759412
186.480396	6212.613575	25.764429
186.300342	6231.992720	25.769447
186.499191	6228.910774	25.774464
186.476010	6249.644124	25.779482
187.169204	6244.104975	25.784500
186.981022	6283.151418	25.789517
187.250044	6266.914588	25.794535
187.758077	6290.625388	25.799552
187.854456	6289.570739	25.804570
188.114234	6297.149179	25.809588
188.179056	6308.358161	25.814605
188.145344	6318.079349	25.819623
188.525071	6316.765523	25.824640
188.905227	6333.194013	25.829658
189.339770	6341.997147	25.834676
189.104955	6338.913510	25.839693
189.278257	6345.125771	25.844711
189.772974	6353.473221	25.849728
189.488709	6365.246154	25.854746
189.930798	6384.685235	25.859764
190.169518	6375.140667	25.864781
190.101680	6419.403450	25.869799
190.610016	6391.184346	25.874816
190.282304	6409.940538	25.879834
191.175033	6391.420055	25.884852
190.908109	6451.693209	25.889869
191.388728	6416.439213	25.894887
191.486275	6443.039428	25.899904
191.551435	6415.736716	25.904922
191.770430	6442.211353	25.909940
192.153308	6444.722307	25.914957
191.907869	6454.050909	25.919975
192.300391	6457.886828	25.924992
192.364409	6480.125860	25.930010
193.090243	6453.375490	25.935028
192.681238	6497.219260	25.940045
192.834476	6482.349976	25.945063
193.044593	6507.569665	25.950080
193.312375	6506.714266	25.955098
193.612139	6503.989107	25.960116
193.686446	6536.383086	25.965133
194.084790	6543.665763	25.970151
194.223307	6547.424972	25.975168
194.388884	6560.446556	25.980186
194.431692	6560.882722	25.985204
194.537193	6565.629100	25.990221
194.859394	6576.723294	25.995239
195.400320	6591.099694	26.000256
195.521142	6604.507681	26.005274
195.736697	6594.524494	26.010292
195.960935	6595.904984	26.015309
195.949501	6624.583482	26.020327
196.391921	6594.517694	26.025344
196.403514	6633.666964	26.030362
196.593024	6605.528969	26.035380
196.711227	6637.619554	26.040397
197.079485	6640.235942	26.045415
197.536393	6627.455003	26.050432
197.323172	6639.443420	26.055450
197.665105	6656.205667	26.060468
197.626692	6662.011216	26.065485
197.758460	6651.482732	26.070503
198.166775	6696.392698	26.075520
198.297984	6683.034209	26.080538
198.498575	6681.019562	26.085556
198.620036	6722.887993	26.090573
198.729197	6702.477872	26.095591
199.038527	6735.542139	26.100608
198.969348	6729.116483	26.105626
199.170059	6768.604175	26.110644
199.757377	6726.202538	26.115661
200.064559	6787.044855	26.120679
200.092742	6770.411563	26.125696
200.615653	6777.788582	26.130714
200.529102	6764.580394	26.135732
200.875746	6803.640504	26.140749
201.036732	6807.695966	26.145767
201.826466	6799.444888	26.150784
201.580633	6806.891766	26.155802
201.777181	6802.426888	26.160820
201.989586	6799.684132	26.165837
201.927757	6796.830886	26.170855
201.655997	6814.137264	26.175872
201.868825	6826.690488	26.180890
202.559467	6830.047029	26.185908
202.481305	6832.325491	26.190925
202.719111	6857.302177	26.195943
202.838503	6863.079499	26.200960
203.133412	6876.325436	26.205978
203.697502	6881.404006	26.210996
203.877413	6887.440774	26.216013
203.430183	6888.619131	26.221031
203.863628	6899.160811	26.226048
204.117243	6925.935286	26.231066
204.554915	6922.720708	26.236084
204.823769	6914.148983	26.241101
204.484321	6950.632731	26.246119
205.037798	6941.150920	26.251136
204.487552	6959.865389	26.256154
205.241671	6966.376355	26.261172
205.617380	6977.357676	26.266189
205.779081	7014.667295	26.271207
205.964064	6993.406741	26.276224
205.952137	7019.154454	26.281242
206.535979	7029.880754	26.286260
206.844297	7019.145258	26.291277
206.795843	7046.292271	26.296295
207.555330	7036.107199	26.301312
207.526839	7064.883684	26.306330
207.903496	7047.465943	26.311348
208.105254	7054.739303	26.316365
208.042782	7062.664565	26.321383
208.016264	7054.121752	26.326400
208.075193	7095.119194	26.331418
208.647091	7054.072393	26.336436
209.004825	7073.912942	26.341453
208.891893	7128.865938	26.346471
209.235700	7118.315122	26.351488
209.362437	7110.522064	26.356506
209.369085	7155.942794	26.361524
209.703655	7140.998307	26.366541
209.663895	7169.683948	26.371559
210.566293	7161.235320	26.376576
210.040749	7173.140986	26.381594
210.304537	7175.938571	26.386612
210.667271	7198.020903	26.391629
210.654654	7210.101327	26.396647
210.943311	7230.396073	26.401664
211.445006	7219.716155	26.406682
211.250409	7254.950126	26.411700
212.019884	7273.811020	26.416717
212.091550	7255.052928	26.421735
212.301432	7283.132481	26.426752
212.347843	7287.925493	26.431770
212.709697	7289.279391	26.436788
213.098316	7296.674149	26.441805
212.922002	7314.011525	26.446823
213.456025	7302.179998	26.451840
213.409637	7333.550064	26.456858
213.768419	7323.623026	26.461876
213.851822	7334.902210	26.466893
214.053786	7340.651606	26.471911
214.309412	7347.246150	26.476928
214.149775	7358.931544	26.481946
214.628988	7384.786494	26.486964
215.060656	7355.164656	26.491981
214.873887	7382.207654	26.496999
215.163209	7408.866367	26.502016
215.572354	7388.850463	26.507034
215.890940	7436.157905	26.512052
216.497069	7425.446243	26.517069
216.257558	7428.176977	26.522087
216.802658	7443.724344	26.527104
216.926177	7460.435773	26.532122
217.118542	7456.215285	26.537140
217.490476	7455.803526	26.542157
217.363220	7458.883031	26.547175
217.524626	7478.272309	26.552192
218.095920	7487.247105	26.557210
218.086229	7481.407268	26.562228
218.353276	7490.328281	26.567245
218.182045	7523.249819	26.572263
218.830278	7495.355679	26.577280
218.584522	7519.803926	26.582298
218.720662	7541.919748	26.587316
218.988738	7532.116402	26.592333
219.199707	7568.377794	26.597351
219.365439	7571.407466	26.602368
219.848781	7586.132359	26.607386
220.018503	7616.224584	26.612404
220.506706	7601.517949	26.617421
220.510336	7624.540995	26.622439
220.857164	7647.469235	26.627456
220.713367	7631.463541	26.632474
220.969128	7679.564676	26.637492
221.643307	7647.938073	26.642509
221.736250	7698.723163	26.647527
221.974113	7680.755566	26.652544
222.208029	7700.648954	26.657562
222.545889	7686.898609	26.662580
222.326307	7723.179445	26.667597
222.558490	7732.211599	26.672615
222.869898	7725.432920	26.677632
223.583558	7748.039637	26.682650
223.195663	7760.988421	26.687668
223.925812	7764.744899	26.692685
224.074253	7768.232951	26.697703
224.357551	7785.657334	26.702720
224.543739	7777.323332	26.707738
224.274784	7792.762428	26.712756
225.014409	7807.921154	26.717773
224.805613	7798.424988	26.722791
225.173095	7821.959224	26.727808
225.192328	7832.378763	26.732826
225.380390	7849.410030	26.737844
226.033138	7853.968079	26.742861
225.796427	7865.918734	26.747879
226.006195	7868.456749	26.752896
226.213396	7885.920920	26.757914
226.354153	7899.828124	26.762932
226.821499	7917.984206	26.767949
226.612344	7929.873079	26.772967
227.155693	7955.498483	26.777984
227.740295	7977.485234	26.783002
227.722527	7972.844871	26.788020
228.287286	7974.622866	26.793037
228.776235	8006.655733	26.798055
228.741132	8001.302873	26.803072
228.868720	7994.701306	26.808090
228.879945	8016.029646	26.813108
229.762705	8030.182212	26.818125
229.243377	8036.230990	26.823143
229.923496	8041.040463	26.828160
230.195034	8045.648328	26.833178
230.151577	8055.403680	26.838196
230.464342	8060.086810	26.843213
230.714553	8081.068697	26.848231
230.954547	8084.420266	26.853248
231.084688	8087.443129	26.858266
231.474694	8095.273202	26.863284
231.688775	8104.779799	26.868301
231.769750	8122.210078	26.873319
232.414157	8130.869885	26.878336
232.673337	8143.172909	26.883354
232.435360	8142.307561	26.888372
232.572778	8151.474681	26.893389
233.023932	8158.637223	26.898407
233.024365	8166.886674	26.903424
233.229233	8179.319564	26.908442
233.256608	8195.800071	26.913460
234.110053	8211.494235	26.918477
234.005005	8240.990229	26.923495
234.026555	8236.864424	26.928512
234.398805	8247.086341	26.933530
234.436970	8284.008879	26.938548
234.786443	8283.368557	26.943565
235.247942	8294.489837	26.948583
235.169904	8302.681054	26.953600
235.693714	8334.668154	26.958618
235.932063	8346.658344	26.963636
236.397819	8336.619947	26.968653
236.352890	8349.830101	26.973671
236.317532	8359.576491	26.978688
236.877199	8369.127313	26.983706
236.806523	8383.332277	26.988724
236.884287	8390.915631	26.993741
237.281700	8424.341024	26.998759
237.597243	8419.936960	27.003776
237.987227	8422.926339	27.008794
238.179660	8467.702178	27.013812
238.800033	8455.189495	27.018829
238.556072	8448.657187	27.023847
238.829663	8473.481380	27.028864
239.338784	8440.677066	27.033882
239.364472	8496.507687	27.038900
239.752424	8480.508377	27.043917
239.872872	8510.495380	27.048935
240.325366	8494.817831	27.053952
240.609431	8513.590087	27.058970
240.655969	8530.472367	27.063988
241.165575	8530.055952	27.069005
240.914535	8526.883158	27.074023
240.874276	8559.996200	27.079040
241.384615	8565.829112	27.084058
241.425078	8579.652217	27.089076
242.014505	8594.428089	27.094093
242.027287	8623.211233	27.099111
242.558942	8632.319738	27.104128
242.648921	8623.853848	27.109146
242.715893	8651.474042	27.114164
243.616391	8647.482241	27.119181
243.856501	8682.582612	27.124199
243.832608	8673.727629	27.129216
244.374029	8674.182736	27.134234
244.509273	8700.153042	27.139252
244.808411	8703.461882	27.144269
245.074836	8704.826410	27.149287
245.103808	8711.534024	27.154304
245.290320	8732.187045	27.159322
245.583222	8753.531734	27.164340
245.861841	8737.649515	27.169357
245.767078	8752.775401	27.174375
245.645953	8798.034221	27.179392
246.349874	8784.083664	27.184410
246.030361	8814.735519	27.189428
246.813232	8824.660243	27.194445
247.024642	8835.800944	27.199463
247.098756	8858.735574	27.204480
247.766721	8858.803821	27.209498
247.427148	8870.787804	27.214516
248.055221	8893.279290	27.219533
248.276940	8894.936608	27.224551
248.666786	8926.392749	27.229568
249.057587	8939.232973	27.234586
249.010961	8942.745316	27.239604
249.049752	8970.144355	27.244621
249.297343	8960.811553	27.249639
249.600204	8995.289655	27.254656
250.435350	9004.536903	27.259674
250.139394	9015.427721	27.264692
250.657611	9020.418352	27.269709
251.030690	9031.910752	27.274727
251.137400	9047.161808	27.279744
251.500626	9040.470676	27.284762
251.628869	9036.590078	27.289780
252.393526	9063.124441	27.294797
252.501454	9067.946386	27.299815
252.511292	9074.212214	27.304832
252.873719	9066.284566	27.309850
252.488611	9090.822905	27.314868
253.008349	9099.655820	27.319885
253.273536	9096.789348	27.324903
253.114933	9125.234075	27.329920
253.687520	9143.531085	27.334938
253.786842	9173.660889	27.339956
254.043470	9172.726864	27.344973
254.332901	9187.097491	27.349991
254.205350	9195.474539	27.355008
254.741740	9212.203565	27.360026
254.927623	9237.512409	27.365044
255.246937	9258.121379	27.370061
255.519386	9274.922453	27.375079
255.481918	9297.671730	27.380096
256.313307	9301.630849	27.385114
256.372709	9332.148600	27.390132
256.530119	9327.010098	27.395149
257.047750	9350.099844	27.400167
257.106307	9351.233948	27.405184
257.875644	9374.408337	27.410202
258.025535	9394.158028	27.415220
258.315438	9394.334551	27.420237
258.502585	9406.696925	27.425255
258.628770	9419.436524	27.430272
259.028598	9414.967981	27.435290
259.063583	9432.194648	27.440308
259.274126	9445.908028	27.445325
259.585258	9454.399827	27.450343
259.556227	9469.270042	27.455360
260.305111	9485.432750	27.460378
260.116293	9501.998735	27.465396
260.557584	9515.667527	27.470413
260.794808	9533.115072	27.475431
261.045394	9552.394858	27.480448
261.111760	9557.647352	27.485466
261.750727	9588.269581	27.490484
261.824125	9590.227231	27.495501
262.250485	9604.449343	27.500519
262.461750	9624.435867	27.505536
262.591331	9657.794183	27.510554
262.886724	9655.801808	27.515572
263.106288	9661.988414	27.520589
263.227728	9684.377316	27.525607
263.643858	9699.387306	27.530624
264.000993	9697.071880	27.535642
264.362422	9733.637196	27.540660
264.531654	9733.905359	27.545677
264.650610	9746.567693	27.550695
264.867378	9760.676598	27.555712
265.319722	9758.850813	27.560730
265.618486	9795.917326	27.565748
265.755776	9804.108484	27.570765
266.264882	9803.374591	27.575783
266.577146	9822.444221	27.580800
266.805443	9825.223184	27.585818
266.793044	9835.743989	27.590836
267.087821	9845.738550	27.595853
267.545005	9854.991103	27.600871
267.523612	9880.365944	27.605888
268.141460	9896.423682	27.610906
268.106105	9914.740636	27.615924
268.075731	9921.831270	27.620941
268.714902	9932.572115	27.625959
268.840742	9948.303444	27.630976
268.994614	9968.174055	27.635994
269.288702	9987.807895	27.641012
269.626819	10004.518658	27.646029
269.934189	10016.296155	27.651047
269.880663	10027.798695	27.656064
270.428142	10037.641750	27.661082
270.628386	10074.348880	27.666100
270.356510	10101.430418	27.671117
271.564595	10102.734695	27.676135
271.862416	10128.988087	27.681152
272.237897	10150.430210	27.686170
272.645832	10146.009348	27.691188
272.688823	10156.019855	27.696205
272.988120	10170.228528	27.701223
273.182141	10175.890969	27.706240
273.540746	10187.334235	27.711258
273.791007	10203.467422	27.716276
273.699025	10219.259332	27.721293
274.574534	10233.833449	27.726311
274.519368	10245.363961	27.731328
274.803687	10256.511414	27.736346
274.787796	10273.550018	27.741364
275.495633	10298.067603	27.746381
275.749268	10291.920665	27.751399
275.930404	10314.657098	27.756416
276.428994	10329.918216	27.761434
276.625514	10324.441037	27.766452
276.190147	10341.608359	27.771469
277.047673	10349.105796	27.776487
277.203115	10376.427818	27.781504
277.503971	10380.930613	27.786522
277.787077	10402.513738	27.791540
278.122740	10427.883349	27.796557
278.741317	10424.514870	27.801575
278.764523	10454.693612	27.806592
279.417089	10443.993672	27.811610
279.377426	10449.207503	27.816628
279.521581	10464.194721	27.821645
279.834242	10466.766366	27.826663
279.742148	10472.906974	27.831680
279.985010	10503.950722	27.836698
280.398604	10519.207875	27.841716
280.502261	10521.951354	27.846733
280.794864	10541.422856	27.851751
280.702559	10557.697596	27.856768
281.315961	10568.322601	27.861786
281.526324	10604.448220	27.866804
281.721706	10616.654850	27.871821
282.064859	10627.013685	27.876839
282.462176	10662.035396	27.881856
282.752424	10675.268935	27.886874
282.763148	10692.463924	27.891892
283.127452	10716.170074	27.896909
283.512783	10728.875775	27.901927
283.383918	10757.602559	27.906944
283.880414	10773.627461	27.911962
284.781492	10791.278375	27.916980
284.515519	10805.694226	27.921997
284.886041	10826.120904	27.927015
285.244315	10839.344531	27.932032
285.607560	10869.573396	27.937050
286.034939	10884.828330	27.942068
286.223553	10908.527372	27.947085
286.947326	10916.358468	27.952103
287.197630	10933.695770	27.957120
287.284914	10942.853312	27.962138
287.852792	10941.531553	27.967156
287.928510	10957.172764	27.972173
288.126467	10974.081665	27.977191
288.532642	10987.125040	27.982208
288.902718	10997.204385	27.987226
289.100854	11015.070705	27.992244
289.329704	11023.207798	27.997261
289.889438	11042.826846	28.002279
289.939115	11053.759266	28.007296
289.978466	11069.296995	28.012314
290.539985	11083.762230	28.017332
290.496315	11107.310511	28.022349
290.955110	11106.888768	28.027367
291.576916	11137.981638	28.032384
291.746760	11145.966470	28.037402
292.190167	11162.732575	28.042420
292.363829	11179.655417	28.047437
292.563621	11185.207532	28.052455
292.658210	11207.839875	28.057472
293.075581	11214.983706	28.062490
293.493624	11227.246637	28.067508
293.629307	11252.642433	28.072525
294.001889	11263.855270	28.077543
294.380789	11276.538850	28.082560
294.756143	11284.781413	28.087578
294.730194	11293.747080	28.092596
295.039353	11306.589763	28.097613
295.716115	11302.295328	28.102631
295.686245	11336.832630	28.107648
295.625451	11339.701637	28.112666
296.244662	11356.357692	28.117684
296.311369	11375.845424	28.122701
296.446423	11388.701760	28.127719
296.886758	11404.013006	28.132736
297.251555	11418.448137	28.137754
297.702483	11418.939816	28.142772
297.741037	11445.504030	28.147789
298.039645	11462.074752	28.152807
298.285244	11479.212738	28.157824
298.298678	11488.625183	28.162842
298.972787	11516.597763	28.167860
299.665165	11538.979489	28.172877
299.578138	11539.876061	28.177895
299.992127	11575.491850	28.182912
299.957209	11584.548054	28.187930
300.430175	11610.558499	28.192948
300.448953	11622.916480	28.197965
301.136342	11639.374273	28.202983
301.239677	11669.624132	28.208000
301.630592	11692.356755	28.213018
302.032844	11697.915356	28.218036
302.385633	11719.523107	28.223053
302.569076	11751.096773	28.228071
302.646624	11757.845228	28.233088
303.136012	11782.302071	28.238106
303.419968	11791.644041	28.243124
303.798371	11811.258955	28.248141
304.588819	11829.875953	28.253159
304.768012	11840.900849	28.258176
304.908490	11849.235466	28.263194
305.296741	11867.431787	28.268212
305.540497	11886.158419	28.273229
305.746621	11911.594663	28.278247
306.011121	11920.977594	28.283264
306.197279	11933.722948	28.288282
306.865668	11949.566660	28.293300
306.903675	11973.284688	28.298317
307.421517	11996.372576	28.303335
307.652139	12009.236247	28.308352
307.990111	12034.914367	28.313370
308.239201	12032.068413	28.318388
308.295447	12052.693241	28.323405
308.604587	12071.750090	28.328423
309.271131	12091.635452	28.333440
309.376582	12096.605752	28.338458
310.236209	12117.211436	28.343476
309.977096	12137.107047	28.348493
310.622493	12151.006436	28.353511
310.952994	12176.972877	28.358528
310.796446	12192.392060	28.363546
311.337685	12200.914074	28.368564
311.686583	12212.507618	28.373581
311.554937	12229.460817	28.378599
311.897341	12244.757634	28.383616
312.130161	12267.802622	28.388634
312.516115	12285.833149	28.393652
312.732838	12316.090234	28.398669
313.262306	12331.416356	28.403687
313.533353	12335.811745	28.408704
313.709782	12359.634249	28.413722
314.316326	12375.985116	28.418740
314.074112	12404.622897	28.423757
314.585161	12418.415257	28.428775
314.911195	12432.759154	28.433792
315.249003	12462.397865	28.438810
315.845663	12477.782887	28.443828
315.783241	12492.922124	28.448845
316.389817	12516.602529	28.453863
316.863585	12526.766337	28.458880
317.051903	12558.351338	28.463898
317.448032	12565.898456	28.468916
317.836506	12591.179860	28.473933
318.128703	12605.267211	28.478951
318.624611	12626.073043	28.483968
318.566753	12640.430308	28.488986
319.005905	12652.743381	28.494004
318.973256	12679.217995	28.499021
319.794564	12696.625509	28.504039
320.207228	12706.127977	28.509056
320.266040	12727.782843	28.514074
320.819324	12745.113687	28.519092
320.970751	12761.429477	28.524109
321.132438	12776.926044	28.529127
321.430790	12792.743827	28.534144
321.833910	12824.078299	28.539162
322.385599	12827.884230	28.544180
322.535188	12859.258788	28.549197
322.893455	12873.884278	28.554215
323.285728	12890.982385	28.559232
323.281217	12915.319067	28.564250
323.912209	12933.966192	28.569268
324.255589	12955.200379	28.574285
324.387675	12975.056382	28.579303
324.794368	12981.358186	28.584320
325.262218	13005.445973	28.589338
325.772303	13018.313781	28.594356
326.068671	13029.791173	28.599373
326.221077	13053.223068	28.604391
326.844538	13061.214741	28.609408
326.927510	13078.177578	28.614426
327.447684	13091.721355	28.619444
327.644259	13108.368983	28.624461
327.704689	13125.123335	28.629479
328.003739	13142.361737	28.634496
327.877226	13174.830777	28.639514
328.623762	13187.804302	28.644532
328.995645	13213.733456	28.649549
329.182412	13223.154380	28.654567
329.551857	13231.916493	28.659584
329.682890	13260.741981	28.664602
330.299055	13267.540457	28.669620
330.247949	13301.114686	28.674637
330.510541	13317.148684	28.679655
330.979814	13339.112892	28.684672
331.381763	13357.543784	28.689690
331.816237	13378.240404	28.694708
332.187998	13405.595803	28.699725
332.289236	13424.342131	28.704743
332.779292	13439.373203	28.709760
333.189999	13472.769521	28.714778
333.687556	13482.577545	28.719796
334.071633	13498.644915	28.724813
334.161411	13507.757170	28.729831
334.585104	13522.711823	28.734848
334.794809	13545.255318	28.739866
335.282513	13560.183572	28.744884
335.855433	13589.591114	28.749901
335.954410	13603.176993	28.754919
336.294428	13623.418581	28.759936
336.491612	13642.847105	28.764954
337.108524	13647.337022	28.769972
337.120345	13683.749386	28.774989
337.586018	13700.160644	28.780007
337.745700	13716.273452	28.785024
337.831976	13756.470075	28.790042
338.214268	13766.670947	28.795060
338.685009	13801.182871	28.800077
338.894745	13831.054640	28.805095
339.430689	13842.872796	28.810112
339.680501	13873.391210	28.815130
340.036281	13889.404663	28.820148
340.229683	13920.707837	28.825165
340.774489	13937.518328	28.830183
341.233070	13972.059932	28.835200
341.315024	13993.034863	28.840218
342.228895	14007.880094	28.845236
342.683903	14018.386186	28.850253
343.190883	14037.293146	28.855271
343.736963	14039.919234	28.860288
344.068659	14061.756852	28.865306
344.302241	14075.149014	28.870324
344.838915	14079.760480	28.875341
345.178546	14105.535515	28.880359
345.541737	14104.206579	28.885376
345.515295	14116.361945	28.890394
345.794014	14116.601730	28.895412
346.179745	14137.584436	28.900429
345.980608	14168.375128	28.905447
346.690191	14169.992884	28.910464
347.083605	14194.067460	28.915482
347.101409	14205.461826	28.920500
347.686675	14222.384461	28.925517
347.687686	14230.992544	28.930535
348.252717	14258.940058	28.935552
348.200815	14292.486779	28.940570
348.784614	14288.318625	28.945588
349.059518	14309.077759	28.950605
348.830383	14341.127662	28.955623
349.498357	14368.990882	28.960640
349.780255	14387.748077	28.965658
350.200515	14407.985400	28.970676
350.767105	14431.132405	28.975693
351.031651	14457.774399	28.980711
351.338011	14483.660859	28.985728
351.501052	14510.669029	28.990746
351.956321	14523.286588	28.995764
352.514397	14569.166235	29.000781
352.627272	14580.127137	29.005799
353.178338	14583.851557	29.010816
353.357239	14624.884500	29.015834
353.343280	14656.176250	29.020852
354.315436	14663.855697	29.025869
354.573350	14691.965124	29.030887
354.965362	14715.747120	29.035904
355.239375	14746.471122	29.040922
355.738571	14774.793763	29.045940
356.311912	14782.840591	29.050957
356.628304	14800.912551	29.055975
356.886512	14834.721889	29.060992
357.377806	14849.251331	29.066010
357.661107	14862.227797	29.071028
358.360134	14881.165030	29.076045
358.514943	14915.752557	29.081063
359.049825	14926.850640	29.086080
359.108720	14941.048384	29.091098
359.810203	14966.097483	29.096116
360.355939	14987.764947	29.101133
360.432331	15008.595833	29.106151
360.853457	15017.754884	29.111168
361.232835	15036.159920	29.116186
361.325289	15057.205979	29.121204
361.783720	15067.540934	29.126221
362.293728	15094.253557	29.131239
362.754814	15089.522891	29.136256
362.473826	15136.271352	29.141274
363.040358	15153.453661	29.146292
363.715759	15165.268930	29.151309
364.078099	15184.950793	29.156327
364.503597	15193.642722	29.161344
364.676664	15212.853121	29.166362
365.367957	15220.243828	29.171380
365.694315	15235.526833	29.176397
366.108398	15263.977209	29.181415
366.156897	15280.429396	29.186432
366.305966	15297.948417	29.191450
366.509175	15314.460417	29.196468
366.996149	15326.998510	29.201485
367.442508	15351.973077	29.206503
368.038969	15364.352542	29.211520
368.071744	15389.898290	29.216538
368.498564	15399.062175	29.221556
368.750263	15419.447756	29.226573
369.010335	15444.334862	29.231591
369.217244	15463.839433	29.236608
369.505133	15496.913465	29.241626
370.109215	15511.265066	29.246644
370.424549	15538.360207	29.251661
370.607989	15563.964600	29.256679
371.102968	15585.267452	29.261696
371.359309	15610.904393	29.266714
371.702676	15634.814840	29.271732
372.040947	15652.943365	29.276749
372.245320	15714.355794	29.281767
372.938483	15704.243079	29.286784
372.957049	15739.044197	29.291802
373.179233	15785.750169	29.296820
373.730375	15807.908005	29.301837
374.027943	15836.155806	29.306855
374.569581	15866.581012	29.311872
375.237733	15888.245697	29.316890
375.727996	15936.364864	29.321908
376.181145	15953.556007	29.326925
376.448417	15958.964796	29.331943
377.000468	15989.589144	29.336960
377.391976	16024.065182	29.341978
377.713720	16040.249284	29.346996
378.537840	16050.293699	29.352013
378.544575	16079.695987	29.357031
378.978023	16108.336545	29.362048
379.361087	16124.923301	29.367066
379.532873	16143.653648	29.372084
379.876339	16156.398727	29.377101
379.993451	16178.166493	29.382119
380.719348	16210.600206	29.387136
381.427363	16230.847330	29.392154
381.927862	16242.624489	29.397172
382.615907	16263.672948	29.402189
382.613489	16281.163104	29.407207
383.126203	16308.816746	29.412224
383.551367	16320.567000	29.417242
383.783230	16345.271407	29.422260
384.139892	16352.774353	29.427277
384.592174	16386.057436	29.432295
385.029450	16388.056790	29.437312
385.031664	16416.946144	29.442330
385.258062	16442.568774	29.447348
385.852992	16459.851953	29.452365
386.031697	16476.706661	29.457383
386.196310	16521.053098	29.462400
386.856995	16523.430202	29.467418
387.229639	16549.702649	29.472436
387.434079	16566.857056	29.477453
387.731500	16602.744087	29.482471
388.104747	16619.513431	29.487488
388.702533	16641.084208	29.492506
388.745068	16664.131119	29.497524
389.590737	16687.063274	29.502541
389.654267	16708.996608	29.507559
389.907779	16724.245369	29.512576
390.610488	16748.927161	29.517594
391.099964	16775.004625	29.522612
391.760360	16801.187166	29.527629
391.836512	16818.732529	29.532647
392.205527	16845.614653	29.537664
392.460578	16870.819302	29.542682
393.013578	16881.697150	29.547700
393.583687	16908.403654	29.552717
393.689780	16926.015424	29.557735
393.975393	16955.260387	29.562752
394.553240	16984.982408	29.567770
394.864224	17008.941291	29.572788
395.362706	17028.767196	29.577805
395.650520	17055.910830	29.582823
395.799476	17068.746908	29.587840
396.674589	17102.393256	29.592858
396.726785	17137.822032	29.597876
397.773825	17163.926457	29.602893
398.251251	17175.152354	29.607911
398.474737	17191.717860	29.612928
398.735436	17215.752197	29.617946
398.865179	17235.603073	29.622964
399.321503	17253.021822	29.627981
399.865354	17293.769796	29.632999
400.486293	17309.815639	29.638016
401.027533	17332.425252	29.643034
401.296051	17353.216886	29.648052
401.700574	17361.951581	29.653069
401.886536	17394.861794	29.658087
402.485649	17413.292736	29.663104
402.868441	17430.401379	29.668122
403.028547	17448.459632	29.673140
403.572505	17466.968124	29.678157
403.495749	17497.630618	29.683175
403.808342	17524.098534	29.688192
404.744504	17558.654793	29.693210
404.884257	17580.540606	29.698228
405.354928	17604.497409	29.703245
405.646480	17627.242510	29.708263
405.875790	17689.035475	29.713280
406.656632	17687.566676	29.718298
406.818182	17708.357526	29.723316
407.645749	17744.165098	29.728333
407.900652	17762.275538	29.733351
408.287749	17774.114464	29.738368
408.892564	17807.284583	29.743386
409.161144	17825.551966	29.748404
409.415114	17852.449647	29.753421
409.647096	17864.770031	29.758439
410.243513	17883.659230	29.763456
410.472314	17911.854276	29.768474
410.435448	17933.649444	29.773492
411.361238	17965.575107	29.778509
411.395844	17979.775780	29.783527
411.941839	18009.989677	29.788544
412.924168	18029.950202	29.793562
412.902147	18063.636091	29.798580
413.786320	18076.367669	29.803597
413.681228	18105.746943	29.808615
413.936080	18126.409711	29.813632
414.827102	18161.933740	29.818650
414.877779	18193.538696	29.823668
415.448075	18216.430402	29.828685
415.510391	18237.770045	29.833703
415.845399	18268.392860	29.838720
416.969007	18296.620436	29.843738
417.266302	18330.354842	29.848756
417.639744	18348.189603	29.853773
417.741921	18375.452925	29.858791
418.315678	18404.171848	29.863808
418.749241	18434.079294	29.868826
418.709643	18458.783484	29.873844
419.556976	18506.517157	29.878861
420.014217	18525.117902	29.883879
419.909196	18549.469668	29.888896
420.990305	18583.197056	29.893914
421.460963	18613.407206	29.898932
421.831455	18633.275450	29.903949
422.357045	18662.543474	29.908967
422.616229	18700.005645	29.913984
423.299097	18710.814297	29.919002
423.321875	18750.312308	29.924020
424.202544	18769.691165	29.929037
424.549251	18786.308628	29.934055
424.735535	18813.873889	29.939072
425.444720	18837.637313	29.944090
425.328652	18870.124951	29.949108
425.975817	18890.838829	29.954125
426.601975	18899.171165	29.959143
426.984394	18942.750246	29.964160
427.871501	18968.378875	29.969178
428.039524	18996.600930	29.974196
428.560843	19004.132288	29.979213
429.207284	19033.336873	29.984231
428.998314	19064.112894	29.989248
429.601449	19093.841439	29.994266
429.890977	19116.055958	29.999284
430.324710	19135.942724	30.004301
430.965756	19163.509377	30.009319
431.410419	19206.143810	30.014336
431.566451	19221.835781	30.019354
432.051928	19248.077708	30.024372
432.826513	19261.243499	30.029389
433.225204	19282.654215	30.034407
433.340019	19314.126417	30.039424
434.036305	19316.975103	30.044442
434.265271	19338.849180	30.049460
434.841066	19364.595788	30.054477
435.048862	19386.613469	30.059495
435.450010	19404.311167	30.064512
435.849564	19424.426989	30.069530
436.058060	19451.527609	30.074548
436.516213	19483.576982	30.079565
437.158333	19502.194328	30.084583
437.277390	19530.931875	30.089600
437.759459	19580.794502	30.094618
437.753853	19600.664454	30.099636
437.951425	19640.637296	30.104653
438.725446	19674.365201	30.109671
439.011375	19720.491145	30.114688
439.910458	19750.213954	30.119706
440.059545	19769.075147	30.124724
440.390776	19825.176059	30.129741
441.333279	19834.573946	30.134759
441.566318	19899.428886	30.139776
442.597578	19915.616021	30.144794
442.739259	19938.334051	30.149812
443.106983	19960.035697	30.154829
443.587456	20000.069906	30.159847
444.098126	20039.802528	30.164864
444.638463	20060.383402	30.169882
444.821799	20090.006703	30.174900
445.616057	20123.847329	30.179917
446.284912	20149.934776	30.184935
446.479109	20166.791028	30.189952
447.072485	20191.782583	30.194970
447.724629	20244.428792	30.199988
448.647364	20234.724881	30.205005
449.053169	20276.143496	30.210023
449.728246	20265.806902	30.215040
450.051320	20286.402216	30.220058
449.894922	20313.636492	30.225076
450.537455	20339.102002	30.230093
451.368018	20352.385019	30.235111
451.333768	20384.945454	30.240128
451.752064	20393.940139	30.245146
451.835935	20424.419390	30.250164
452.302894	20444.444285	30.255181
452.713334	20472.715828	30.260199
453.033255	20511.613401	30.265216
453.755445	20517.141992	30.270234
453.993290	20566.157587	30.275252
454.415580	20599.823046	30.280269
454.913181	20617.659533	30.285287
455.320082	20673.417923	30.290304
455.849092	20690.351729	30.295322
456.233180	20721.714562	30.300340
456.772658	20739.991035	30.305357
457.120474	20762.437229	30.310375
457.265666	20800.746735	30.315392
458.277816	20825.196928	30.320410
458.412125	20843.143921	30.325428
458.703734	20883.193551	30.330445
459.447589	20909.997988	30.335463
459.747972	20936.757360	30.340480
460.180174	20957.894131	30.345498
460.835852	20986.865047	30.350516
461.057165	21024.096270	30.355533
461.693455	21041.910358	30.360551
462.064091	21078.942303	30.365568
462.679986	21099.409738	30.370586
463.151666	21135.684654	30.375604
463.513342	21169.100322	30.380621
464.110013	21196.591804	30.385639
464.446396	21217.964701	30.390656
464.549702	21242.354797	30.395674
465.134830	21302.086138	30.400692
465.714536	21315.982883	30.405709
466.456956	21340.111439	30.410727
466.506009	21400.021488	30.415744
467.426964	21416.559720	30.420762
467.692201	21451.144319	30.425780
468.205624	21494.230420	30.430797
468.749062	21493.070446	30.435815
468.906497	21538.652423	30.440832
469.594695	21585.992847	30.445850
470.049678	21614.436161	30.450868
470.632534	21638.336218	30.455885
471.178736	21662.490232	30.460903
471.651518	21698.374069	30.465920
472.396333	21716.470123	30.470938
472.659244	21753.367246	30.475956
473.047857	21782.870471	30.480973
473.268837	21814.498530	30.485991
474.041139	21842.564865	30.491008
474.223538	21881.050246	30.496026
474.595488	21914.921077	30.501044
475.096356	21948.814760	30.506061
475.904740	21979.974687	30.511079
476.229871	22017.215348	30.516096
476.854339	22038.314282	30.521114
477.631574	22068.769742	30.526132
478.347720	22100.869220	30.531149
478.880013	22109.287949	30.536167
479.043045	22139.041214	30.541184
479.426016	22162.379291	30.546202
480.330182	22197.126005	30.551220
480.509065	22223.752559	30.556237
480.761469	22253.253163	30.561255
480.942490	22292.613990	30.566272
481.338187	22305.280001	30.571290
481.773985	22338.282311	30.576308
481.881737	22379.306605	30.581325
483.136521	22397.667958	30.586343
483.717840	22422.761086	30.591360
484.063702	22442.139947	30.596378
484.573948	22470.484645	30.601396
484.738226	22504.505605	30.606413
485.375504	22508.716222	30.611431
485.853812	22539.996792	30.616448
486.535933	22581.944541	30.621466
487.019011	22585.115692	30.626484
487.365551	22631.741842	30.631501
487.962847	22654.774782	30.636519
487.951903	22674.135160	30.641536
488.617667	22705.249938	30.646554
489.435191	22747.267919	30.651572
489.482295	22775.749957	30.656589
490.128869	22795.402694	30.661607
490.680686	22839.439373	30.666624
490.969804	22878.469392	30.671642
491.743531	22903.312889	30.676660
491.939672	22939.452343	30.681677
492.454768	22986.303151	30.686695
492.979850	23019.254069	30.691712
493.403965	23044.217281	30.696730
493.991026	23079.114127	30.701748
494.593952	23117.011755	30.706765
494.750309	23160.599581	30.711783
495.085115	23191.860195	30.716800
495.656146	23228.939307	30.721818
496.297373	23267.801562	30.726836
497.093428	23310.476627	30.731853
497.519909	23322.044522	30.736871
497.965276	23371.357139	30.741888
498.587158	23412.514083	30.746906
499.203654	23434.801568	30.751924
499.683341	23476.361763	30.756941
500.586080	23495.060895	30.761959
500.774818	23521.550226	30.766976
501.084280	23562.972359	30.771994
502.304908	23586.676111	30.777012
502.770900	23609.681742	30.782029
502.922597	23632.081356	30.787047
503.266968	23666.090301	30.792064
503.779025	23705.329441	30.797082
504.615684	23727.108884	30.802100
504.791478	23757.243599	30.807117
505.412933	23769.604658	30.812135
505.750594	23827.309490	30.817152
506.319432	23859.182389	30.822170
506.813261	23883.046477	30.827188
507.201532	23914.460685	30.832205
507.772056	23968.370177	30.837223
508.094605	23997.365838	30.842240
508.562970	24020.496139	30.847258
509.222988	24040.820175	30.852276
509.428633	24078.581748	30.857293
510.344191	24107.457939	30.862311
510.656742	24125.804436	30.867328
510.575513	24179.148150	30.872346
511.515033	24206.142870	30.877364
511.614450	24235.262730	30.882381
512.413677	24276.967892	30.887399
512.964706	24307.604710	30.892416
513.478898	24339.983524	30.897434
513.835023	24377.121614	30.902452
514.239593	24409.685024	30.907469
515.043564	24438.080984	30.912487
515.382624	24498.625307	30.917504
515.859351	24527.562717	30.922522
516.653507	24562.243157	30.927540
517.055388	24596.436344	30.932557
517.368350	24632.620908	30.937575
517.982857	24680.185572	30.942592
518.355328	24709.782689	30.947610
519.257153	24739.901288	30.952628
519.231914	24796.900214	30.957645
520.363208	24822.256139	30.962663
520.833177	24870.064166	30.967680
521.408346	24915.805147	30.972698
522.035660	24926.787675	30.977716
522.434767	24970.126743	30.982733
522.850243	25004.644757	30.987751
523.486679	25041.148164	30.992768
523.758315	25083.435751	30.997786
524.410392	25119.601275	31.002804
525.074907	25160.279384	31.007821
525.955537	25191.855581	31.012839
526.717537	25232.337167	31.017856
526.883891	25259.618328	31.022874
527.636123	25287.865716	31.027892
527.856663	25325.234788	31.032909
528.236367	25359.898700	31.037927
528.756618	25396.714468	31.042944
529.332701	25441.126313	31.047962
530.180278	25463.828860	31.052980
530.282585	25492.284120	31.057997
531.340431	25543.033349	31.063015
531.327952	25575.782160	31.068032
532.142359	25613.118753	31.073050
532.909135	25634.128140	31.078068
532.948791	25666.553731	31.083085
533.641389	25706.544201	31.088103
533.896764	25751.379816	31.093120
534.645785	25780.869313	31.098138
535.586324	25815.197521	31.103156
535.705213	25866.475469	31.108173
536.234128	25891.441432	31.113191
537.420244	25928.614782	31.118208
537.386369	25967.969305	31.123226
537.783657	25995.704930	31.128244
537.870121	26026.049588	31.133261
538.505199	26068.415810	31.138279
539.106455	26095.653542	31.143296
539.646095	26130.205417	31.148314
539.881853	26169.136200	31.153332
540.145996	26222.833481	31.158349
541.088420	26269.120130	31.163367
541.556944	26297.115140	31.168384
541.613940	26343.840824	31.173402
542.553589	26372.220991	31.178420
543.272538	26446.124314	31.183437
543.849792	26470.426461	31.188455
544.731988	26508.437368	31.193472
545.163929	26550.086450	31.198490
545.974826	26583.042556	31.203508
546.133659	26622.990350	31.208525
546.773484	26653.312651	31.213543
547.474019	26689.999478	31.218560
548.046249	26731.778732	31.223578
548.567135	26764.072377	31.228596
549.064734	26805.835351	31.233613
549.464986	26838.972412	31.238631
550.346391	26890.534747	31.243648
550.636410	26924.733399	31.248666
551.531185	26963.428784	31.253684
551.849871	26999.683966	31.258701
552.732033	27029.225464	31.263719
553.316330	27073.657073	31.268736
553.648313	27116.818837	31.273754
554.412602	27155.319605	31.278772
555.146944	27182.649862	31.283789
555.594097	27209.911673	31.288807
555.874855	27258.163489	31.293824
556.502655	27304.321252	31.298842
557.092341	27324.632327	31.303860
557.400027	27364.054036	31.308877
557.884720	27404.527776	31.313895
558.308767	27458.207652	31.318912
558.969017	27490.872119	31.323930
559.417268	27523.869013	31.328948
559.864297	27571.015144	31.333965
560.428580	27632.298855	31.338983
561.073142	27659.243206	31.344000
561.282859	27715.565083	31.349018
561.923169	27766.172777	31.354036
562.518908	27789.645940	31.359053
563.286463	27855.248684	31.364071
564.270043	27887.394467	31.369088
564.715803	27927.882813	31.374106
565.514429	27973.477173	31.379124
565.685743	28011.770320	31.384141
566.588641	28060.452528	31.389159
566.981926	28099.314039	31.394176
567.367589	28147.267380	31.399194
568.449143	28174.870993	31.404212
568.602229	28203.903626	31.409229
569.176680	28242.467171	31.414247
569.788016	28271.869729	31.419264
570.013179	28319.570234	31.424282
570.682611	28359.319668	31.429300
571.640843	28405.367288	31.434317
571.987505	28427.596794	31.439335
572.590938	28468.995822	31.444352
573.065948	28498.411051	31.449370
573.515616	28542.865001	31.454388
573.953635	28593.904608	31.459405
574.232122	28628.450656	31.464423
574.909957	28665.339426	31.469440
575.520662	28732.630035	31.474458
576.182709	28766.399869	31.479476
576.716421	28818.788023	31.484493
577.246840	28858.956357	31.489511
577.681568	28901.476983	31.494528
578.275219	28962.658630	31.499546
579.131636	29000.750448	31.504564
579.784150	29044.075107	31.509581
580.224299	29089.463394	31.514599
580.962593	29141.777460	31.519616
581.571550	29189.630562	31.524634
582.201592	29235.052046	31.529652
582.687626	29281.021356	31.534669
583.681938	29311.894975	31.539687
584.001445	29377.778537	31.544704
584.436767	29398.532845	31.549722
585.015440	29481.229547	31.554740
585.847770	29514.077142	31.559757
586.119177	29550.785245	31.564775
587.153053	29604.144243	31.569792
587.515014	29642.609438	31.574810
588.312331	29680.573589	31.579828
589.002250	29721.407325	31.584845
589.489794	29787.265782	31.589863
590.432497	29815.253630	31.594880
590.503333	29852.126734	31.599898
591.457859	29906.482737	31.604916
591.894279	29944.058996	31.609933
592.372348	29993.547486	31.614951
592.914569	30015.937136	31.619968
593.261934	30098.680117	31.624986
594.179363	30123.191264	31.630004
594.349284	30161.202878	31.635021
594.730736	30225.510357	31.640039
595.804743	30263.676078	31.645056
595.973219	30322.327070	31.650074
596.827893	30363.244920	31.655092
597.557371	30425.379658	31.660109
597.742949	30465.502869	31.665127
598.937246	30524.369448	31.670144
599.602974	30572.430334	31.675162
600.109824	30593.116464	31.680180
600.837463	30635.930661	31.685197
601.414691	30682.814515	31.690215
602.126740	30703.756515	31.695232
602.327863	30760.922440	31.700250
603.043165	30776.943723	31.705268
603.795394	30829.260997	31.710285
604.097059	30873.070353	31.715303
604.594011	30897.712676	31.720320
605.122748	30970.128744	31.725338
605.743194	30997.068310	31.730356
606.351553	31060.773992	31.735373
606.654347	31085.663438	31.740391
607.811315	31156.943248	31.745408
607.943031	31196.296686	31.750426
608.616737	31248.333087	31.755444
609.367789	31276.656579	31.760461
610.116147	31353.346728	31.765479
610.468514	31369.557209	31.770496
611.412357	31445.253680	31.775514
612.121963	31471.213697	31.780532
612.575333	31518.890374	31.785549
613.101449	31573.194074	31.790567
613.788960	31608.045373	31.795584
614.341570	31694.782762	31.800602
615.064098	31704.879263	31.805620
615.679358	31781.570547	31.810637
616.314094	31821.376523	31.815655
616.831351	31857.149120	31.820672
617.509246	31916.441821	31.825690
618.137326	31974.957760	31.830708
618.627846	32003.281448	31.835725
619.147061	32075.461188	31.840743
620.157761	32115.152840	31.845760
620.841803	32156.551557	31.850778
621.107155	32221.006720	31.855796
622.117107	32270.466253	31.860813
622.579385	32314.543891	31.865831
623.356631	32348.819788	31.870848
623.787814	32420.337313	31.875866
624.296159	32464.739012	31.880884
624.899109	32519.561620	31.885901
625.516335	32568.750444	31.890919
626.021759	32606.518850	31.895936
626.490767	32676.094330	31.900954
626.837755	32727.586921	31.905972
628.015176	32782.928910	31.910989
628.429816	32840.175246	31.916007
629.286466	32888.280296	31.921024
629.956634	32944.625691	31.926042
630.802573	33000.364814	31.931060
631.491180	33028.784822	31.936077
631.703692	33117.982880	31.941095
632.897085	33136.893667	31.946112
632.669970	33204.545736	31.951130
634.022770	33227.975547	31.956148
634.369157	33298.864123	31.961165
634.715297	33322.153312	31.966183
635.773750	33391.789262	31.971200
636.262836	33423.622800	31.976218
636.731178	33465.976544	31.981236
637.142672	33525.574393	31.986253
637.643922	33584.502431	31.991271
638.367581	33621.382490	31.996288
638.795153	33677.542033	32.001306
639.597518	33744.036152	32.006324
640.450734	33788.851502	32.011341
640.916764	33834.731157	32.016359
641.725704	33894.974804	32.021376
642.555881	33946.424197	32.026394
643.063927	34000.010514	32.031412
643.616597	34042.580871	32.036429
643.905503	34109.569642	32.041447
644.614538	34160.049056	32.046464
645.293604	34226.418147	32.051482
646.064271	34280.720192	32.056500
647.044759	34335.762991	32.061517
647.514159	34391.341349	32.066535
648.454955	34443.796149	32.071552
648.881304	34503.095638	32.076570
649.850801	34556.370663	32.081588
650.353988	34602.602785	32.086605
650.854745	34672.205244	32.091623
651.812213	34716.662855	32.096640
652.428697	34767.184077	32.101658
652.800920	34831.003404	32.106676
653.640725	34871.668444	32.111693
654.412146	34931.061115	32.116711
655.077172	34978.184403	32.121728
655.209358	35040.289788	32.126746
655.943531	35092.155280	32.131764
657.148930	35148.588469	32.136781
657.449417	35211.618276	32.141799
658.271504	35257.030563	32.146816
659.029411	35302.491029	32.151834
659.411297	35381.231933	32.156852
660.434835	35422.885874	32.161869
661.612987	35476.373400	32.166887
662.026984	35521.239725	32.171904
662.362165	35574.786127	32.176922
662.720861	35634.541827	32.181940
663.618596	35672.437625	32.186957
664.343244	35735.118103	32.191975
665.495217	35779.109325	32.196992
666.299454	35835.651290	32.202010
666.151689	35886.363814	32.207028
667.268737	35923.003478	32.212045
667.934753	35978.576319	32.217063
668.500697	36036.889487	32.222080
669.132476	36085.282408	32.227098
669.735281	36124.670284	32.232116
670.673755	36166.133108	32.237133
670.860481	36220.696849	32.242151
671.625409	36251.946409	32.247168
672.387912	36297.951184	32.252186
672.905724	36345.546362	32.257204
673.265105	36398.161389	32.262221
673.804304	36458.887668	32.267239
674.968202	36491.095752	32.272256
675.533014	36537.638738	32.277274
675.977854	36601.065432	32.282292
677.027133	36655.608335	32.287309
677.380454	36705.116301	32.292327
678.299986	36744.603404	32.297344
678.870849	36796.768217	32.302362
679.167326	36874.574339	32.307380
680.199826	36922.585829	32.312397
680.722316	36980.373160	32.317415
681.497110	37027.530478	32.322432
682.256631	37091.684609	32.327450
682.341999	37150.945309	32.332468
683.343610	37202.725898	32.337485
683.729517	37268.114773	32.342503
684.686679	37326.958218	32.347520
685.705313	37382.509528	32.352538
686.248846	37447.831434	32.357556
686.851607	37493.566943	32.362573
687.519264	37551.738323	32.367591
688.286470	37621.534512	32.372608
689.290493	37682.041421	32.377626
689.674944	37739.820231	32.382644
690.603827	37802.198430	32.387661
691.114891	37866.291016	32.392679
691.692633	37922.893431	32.397696
692.609932	37968.386217	32.402714
693.293598	38041.733965	32.407732
694.155859	38091.866608	32.412749
695.031075	38148.226904	32.417767
695.779382	38204.885098	32.422784
696.228779	38255.369348	32.427802
696.633835	38326.273058	32.432820
697.285935	38387.174377	32.437837
697.960660	38450.725958	32.442855
698.679207	38515.579495	32.447872
699.727834	38567.709993	32.452890
700.446916	38636.690254	32.457908
700.836577	38691.556077	32.462925
701.452490	38750.704807	32.467943
702.310735	38803.317298	32.472960
702.943093	38858.485602	32.477978
703.467358	38922.351461	32.482996
704.553205	38985.845903	32.488013
705.340879	39049.411710	32.493031
706.341819	39109.876931	32.498048
707.306533	39158.774415	32.503066
707.864345	39205.073602	32.508084
708.557033	39241.497962	32.513101
708.798250	39296.067708	32.518119
709.392176	39324.586062	32.523136
710.226476	39381.559333	32.528154
710.673529	39441.833253	32.533172
711.733389	39494.330646	32.538189
712.029500	39548.209695	32.543207
712.662532	39604.895663	32.548224
713.552239	39654.270113	32.553242
713.806723	39717.067087	32.558260
714.941390	39775.662170	32.563277
715.385156	39840.942977	32.568295
716.132866	39904.849495	32.573312
716.793214	39968.186719	32.578330
717.182798	40031.868472	32.583348
718.056227	40089.954324	32.588365
718.816516	40156.985177	32.593383
719.394776	40231.469320	32.598400
720.235483	40294.842120	32.603418
720.896821	40364.100366	32.608436
721.635093	40441.127163	32.613453
722.597016	40507.977489	32.618471
723.180577	40570.766217	32.623488
724.011521	40634.198604	32.628506
724.291429	40705.289863	32.633524
725.597548	40772.622589	32.638541
726.585863	40829.077876	32.643559
727.047451	40904.354663	32.648576
728.342181	40963.136516	32.653594
728.864691	41029.831763	32.658612
729.866476	41086.844007	32.663629
730.513351	41143.625936	32.668647
731.253260	41204.720501	32.673664
731.950071	41256.025852	32.678682
732.428603	41316.742950	32.683700
733.233020	41376.143621	32.688717
734.181995	41440.590000	32.693735
734.663788	41512.384204	32.698752
735.486387	41567.650859	32.703770
736.079371	41635.955275	32.708788
737.084802	41699.844835	32.713805
737.793348	41764.198238	32.718823
738.372224	41814.498964	32.723840
739.463752	41877.240007	32.728858
739.968415	41948.890464	32.733876
740.881073	42011.805566	32.738893
741.567447	42065.464831	32.743911
742.216431	42126.533003	32.748928
743.278183	42171.648182	32.753946
744.007752	42233.754241	32.758964
744.574384	42285.414590	32.763981
745.413973	42356.899878	32.768999
746.124347	42414.865041	32.774016
746.948903	42478.363637	32.779034
747.345039	42529.808988	32.784052
748.361047	42560.574458	32.789069
748.748140	42617.109282	32.794087
749.152586	42681.829961	32.799104
750.082203	42733.929089	32.804122
750.724759	42788.799363	32.809140
751.532665	42854.178789	32.814157
752.100609	42924.835947	32.819175
752.800648	42988.668525	32.824192
753.458909	43044.391930	32.829210
753.907423	43105.164288	32.834228
754.707928	43199.026650	32.839245
755.906571	43256.071552	32.844263
756.007217	43326.770049	32.849280
756.885576	43415.977968	32.854298
757.859071	43466.946214	32.859316
758.747718	43550.437428	32.864333
759.640269	43625.559739	32.869351
760.076334	43689.222430	32.874368
761.079098	43746.369535	32.879386
761.815418	43837.813508	32.884404
762.567015	43903.653808	32.889421
763.479333	43952.563893	32.894439
764.260700	44037.348948	32.899456
765.064057	44106.061834	32.904474
765.630821	44179.837812	32.909492
766.523855	44254.306635	32.914509
767.648752	44321.051230	32.919527
768.168632	44380.911353	32.924544
769.088614	44441.670133	32.929562
769.732912	44519.914707	32.934580
770.491418	44583.983616	32.939597
771.557933	44653.035331	32.944615
772.225051	44731.207822	32.949632
773.194150	44796.408048	32.954650
773.789481	44862.674350	32.959668
774.785982	44946.719806	32.964685
775.692364	44994.908209	32.969703
776.179773	45067.075934	32.974720
776.986501	45128.337814	32.979738
777.716992	45188.123026	32.984756
778.463225	45261.010637	32.989773
779.577861	45313.908319	32.994791
780.299349	45397.211048	32.999808
781.298673	45451.196963	33.004826
781.991593	45522.377968	33.009844
782.647777	45593.804876	33.014861
783.515127	45660.576691	33.019879
784.062815	45721.515939	33.024896
785.075668	45778.450456	33.029914
785.049765	45858.662762	33.034932
785.925457	45937.454205	33.039949
787.200916	45996.805255	33.044967
787.745221	46070.286801	33.049984
788.163172	46145.542881	33.055002
789.150092	46211.029508	33.060020
789.792273	46277.867921	33.065037
790.975659	46358.543085	33.070055
791.853771	46402.941367	33.075072
792.567920	46471.611542	33.080090
793.316600	46516.295729	33.085108
794.031637	46582.401227	33.090125
794.790597	46657.097276	33.095143
795.332689	46717.971478	33.100160
795.993863	46770.863735	33.105178
796.798025	46871.932409	33.110196
797.704142	46913.377596	33.115213
798.777450	47010.681307	33.120231
798.876214	47064.597864	33.125248
799.819076	47150.164266	33.130266
800.568490	47208.584084	33.135284
801.639382	47303.428848	33.140301
802.584123	47366.471853	33.145319
803.550617	47438.446896	33.150336
803.549589	47526.550639	33.155354
804.895820	47584.883020	33.160372
805.731242	47662.085819	33.165389
807.077948	47741.905240	33.170407
807.387314	47804.407298	33.175424
808.475824	47883.735236	33.180442
809.293868	47946.655351	33.185460
809.722343	48025.795554	33.190477
811.160243	48101.781127	33.195495
811.899865	48159.129727	33.200512
813.229616	48233.943560	33.205530
814.014588	48306.367539	33.210548
814.750605	48359.350477	33.215565
815.627383	48435.590880	33.220583
816.360127	48488.618901	33.225600
816.987532	48565.745178	33.230618
817.683563	48630.062869	33.235636
818.244271	48696.150389	33.240653
819.568751	48772.895258	33.245671
820.189824	48847.322792	33.250688
820.595901	48903.789759	33.255706
822.024238	49001.849424	33.260724
821.668976	49062.442267	33.265741
823.526065	49114.567466	33.270759
823.910901	49237.731753	33.275776
824.724191	49279.676919	33.280794
825.860575	49388.958612	33.285812
826.230236	49432.871183	33.290829
827.274941	49525.848245	33.295847
828.232948	49586.337977	33.300864
829.111604	49683.289816	33.305882
830.289450	49732.277932	33.310900
830.937682	49828.475204	33.315917
831.963420	49878.791172	33.320935
832.572175	49944.875698	33.325952
833.326544	50028.128842	33.330970
834.329963	50080.257077	33.335988
834.842978	50154.656801	33.341005
835.707480	50221.380102	33.346023
836.057683	50270.179561	33.351040
837.030603	50354.999346	33.356058
837.865517	50423.451088	33.361076
838.410619	50491.150838	33.366093
839.569396	50580.252738	33.371111
839.974484	50654.340380	33.376128
840.528713	50703.297892	33.381146
841.808514	50808.671358	33.386164
842.448124	50882.296597	33.391181
843.702027	50971.492606	33.396199
844.416342	51042.840797	33.401216
845.492547	51114.204258	33.406234
845.908789	51181.280202	33.411252
846.822312	51283.514808	33.416269
848.059431	51334.132608	33.421287
848.675525	51440.975587	33.426304
849.761953	51487.048175	33.431322
850.920555	51583.972102	33.436340
851.027716	51685.630431	33.441357
852.162742	51719.713072	33.446375
852.887419	51840.748884	33.451392
853.800037	51888.983554	33.456410
854.953681	51998.407879	33.461428
855.999408	52060.637270	33.466445
856.736812	52155.030832	33.471463
857.445252	52210.753211	33.476480
858.166176	52311.645178	33.481498
859.176114	52389.939010	33.486516
860.062142	52455.117629	33.491533
861.077159	52545.457784	33.496551
861.724882	52621.736770	33.501568
862.643289	52695.804799	33.506586
863.370372	52797.272906	33.511604
864.166694	52869.016126	33.516621
865.114815	52974.499292	33.521639
866.084228	53042.803923	33.526656
866.968782	53126.312700	33.531674
867.836194	53203.761666	33.536692
869.002449	53290.584494	33.541709
869.863795	53364.923158	33.546727
870.762092	53443.671731	33.551744
871.407545	53544.421639	33.556762
872.289874	53586.994015	33.561780
872.828855	53715.971931	33.566797
874.157799	53767.121698	33.571815
875.166439	53864.839267	33.576832
875.913176	53937.879215	33.581850
877.316232	53990.179324	33.586868
877.755465	54123.657914	33.591885
878.741392	54156.001393	33.596903
879.417769	54275.287377	33.601920
880.251780	54320.899236	33.606938
880.955159	54415.310023	33.611956
881.775982	54473.524482	33.616973
882.840456	54545.903982	33.621991
883.711559	54613.002364	33.627008
884.577212	54674.808602	33.632026
885.687273	54766.899681	33.637044
886.289930	54814.288777	33.642061
887.143931	54919.662524	33.647079
887.991538	54966.940438	33.652096
888.442586	55081.352997	33.657114
889.624193	55151.377335	33.662132
890.395263	55228.361030	33.667149
891.063504	55304.610168	33.672167
892.235997	55404.506864	33.677184
892.697905	55477.838223	33.682202
893.878838	55590.240748	33.687220
894.223340	55667.047966	33.692237
895.681562	55741.468674	33.697255
896.410273	55848.793233	33.702272
897.043830	55910.463830	33.707290
898.165478	56036.944349	33.712308
898.872127	56103.758729	33.717325
899.979126	56224.725084	33.722343
901.015610	56284.280997	33.727360
901.824775	56379.471123	33.732378
902.621135	56509.479017	33.737396
903.354259	56584.296335	33.742413
904.712921	56663.029773	33.747431
905.042953	56782.769213	33.752448
906.363037	56848.481688	33.757466
907.378190	56979.888107	33.762484
908.347613	57055.465252	33.767501
909.228025	57156.816450	33.772519
910.340265	57211.429224	33.777536
910.894949	57339.088571	33.782554
912.076376	57436.220060	33.787572
913.280493	57503.920061	33.792589
913.925809	57636.059272	33.797607
914.554636	57713.666379	33.802624
915.164135	57800.220449	33.807642
917.077296	57866.883979	33.812660
917.462361	57968.643629	33.817677
918.680578	58057.596035	33.822695
919.915643	58151.246937	33.827712
920.119403	58247.853208	33.832730
921.465972	58370.465599	33.837748
921.851076	58482.668338	33.842765
922.880260	58548.016445	33.847783
924.088447	58628.206066	33.852800
925.007944	58748.808415	33.857818
925.937411	58877.741565	33.862836
926.971671	58976.138998	33.867853
928.009954	59040.095103	33.872871
929.154295	59104.277654	33.877888
929.685987	59205.881849	33.882906
930.723035	59316.132633	33.887924
931.465655	59403.332861	33.892941
932.289020	59464.375807	33.897959
933.428739	59526.991425	33.902976
934.056074	59637.842879	33.907994
935.142952	59706.560976	33.913012
935.979091	59801.925464	33.918029
936.930157	59884.699870	33.923047
938.276367	59961.283468	33.928064
938.328093	60076.210463	33.933082
939.681518	60134.487553	33.938100
940.823594	60254.672742	33.943117
941.608839	60327.327811	33.948135
943.103777	60426.502627	33.953152
943.596665	60519.175330	33.958170
945.045425	60581.069642	33.963188
945.666073	60703.999217	33.968205
946.636895	60758.190294	33.973223
947.881171	60861.126749	33.978240
948.400500	60947.065699	33.983258
949.145416	61046.985166	33.988276
950.313729	61130.021014	33.993293
951.070018	61236.159931	33.998311
952.394262	61315.426989	34.003328
952.883582	61438.849589	34.008346
954.229593	61505.515411	34.013364
954.743391	61610.359382	34.018381
955.709459	61710.092471	34.023399
956.935258	61794.918782	34.028416
957.961517	61913.241637	34.033434
959.101106	61989.361202	34.038452
959.689732	62112.210359	34.043469
960.301675	62184.319192	34.048487
961.626349	62317.352875	34.053504
962.681149	62393.727551	34.058522
963.728709	62512.533908	34.063540
964.531180	62605.565514	34.068557
965.352218	62721.039922	34.073575
967.119127	62775.504882	34.078592
967.674542	62908.652498	34.083610
968.741108	63022.163432	34.088628
969.296168	63096.659468	34.093645
971.138800	63167.218385	34.098663
972.002338	63299.773422	34.103680
972.372010	63392.464079	34.108698
973.768183	63455.604652	34.113716
974.456236	63553.733831	34.118733
975.508897	63701.972109	34.123751
976.440263	63783.614182	34.128768
977.475454	63853.505172	34.133786
978.309989	63981.354776	34.138804
979.042182	64090.355732	34.143821
980.252555	64179.174262	34.148839
981.663692	64274.049912	34.153856
982.068047	64393.800953	34.158874
983.112452	64465.840192	34.163892
984.012408	64555.688861	34.168909
984.929681	64648.914337	34.173927
986.282696	64744.970070	34.178944
987.272716	64832.235029	34.183962
988.354677	64900.480213	34.188980
989.336362	65003.484177	34.193997
990.148453	65103.171199	34.199015
991.266924	65199.405495	34.204032
992.123375	65281.245924	34.209050
993.462117	65361.421403	34.214068
993.980979	65453.930965	34.219085
994.693492	65573.160320	34.224103
995.944685	65637.373426	34.229120
996.552236	65747.878570	34.234138
997.317130	65855.617936	34.239156
998.559654	65966.932904	34.244173
999.374011	66053.413384	34.249191
1000.422162	66188.469970	34.254208
1001.141140	66281.927608	34.259226
1002.550896	66380.493410	34.264244
1003.741099	66505.776617	34.269261
1004.504195	66597.807499	34.274279
1005.748481	66725.070160	34.279296
1006.994045	66825.742604	34.284314
1007.864524	66921.042716	34.289332
1008.597641	67017.821204	34.294349
1009.676264	67158.650259	34.299367
1010.948863	67247.416274	34.304384
1011.566594	67353.721891	34.309402
1013.045473	67475.437409	34.314420
1014.032222	67575.393732	34.319437
1014.764688	67705.296390	34.324455
1015.901094	67798.761298	34.329472
1016.952370	67910.181087	34.334490
1017.630266	68020.384832	34.339508
1018.845157	68128.848645	34.344525
1020.121041	68240.544149	34.349543
1021.250790	68344.171007	34.354560
1022.088928	68456.550176	34.359578
1023.270641	68580.802651	34.364596
1024.695011	68660.081170	34.369613
1025.318741	68786.407407	34.374631
1026.842014	68889.854540	34.379648
1027.544502	68998.670061	34.384666
1028.709842	69097.835071	34.389684
1029.548111	69222.436887	34.394701
1030.720991	69321.930355	34.399719
1031.788173	69424.871660	34.404736
1032.955347	69542.915962	34.409754
1033.926313	69623.843655	34.414772
1035.054296	69747.619331	34.419789
1036.122913	69822.530393	34.424807
1037.252547	69952.473312	34.429824
1038.387646	70017.385982	34.434842
1039.293879	70144.010907	34.439860
1040.035347	70202.517241	34.444877
1041.105681	70318.086033	34.449895
1042.395010	70402.359068	34.454912
1043.036409	70497.741581	34.459930
1044.193708	70584.633122	34.464948
1045.342000	70698.763870	34.469965
1046.170517	70785.253696	34.474983
1047.054493	70895.093382	34.480000
1048.007394	70999.242642	34.485018
1048.995156	71088.842306	34.490036
1049.839253	71218.409386	34.495053
1051.387631	71292.302006	34.500071
1052.037746	71412.196298	34.505088
1053.147006	71509.676486	34.510106
1054.268019	71608.494788	34.515124
1055.510858	71736.264280	34.520141
1056.063905	71825.538381	34.525159
1057.288696	71947.972999	34.530176
1058.855138	72048.327553	34.535194
1059.734954	72175.721652	34.540212
1060.922871	72245.467006	34.545229
1061.497498	72390.950680	34.550247
1062.742604	72477.135229	34.555264
1063.977424	72573.987782	34.560282
1064.745804	72727.101387	34.565300
1066.200620	72808.495991	34.570317
1066.629201	72966.701569	34.575335
1067.464930	73071.493309	34.580352
1069.082905	73157.533041	34.585370
1070.114835	73299.588970	34.590388
1071.303404	73412.319851	34.595405
1072.229646	73534.318866	34.600423
1073.537666	73636.441338	34.605440
1074.606616	73757.028825	34.610458
1075.676219	73885.282043	34.615476
1076.983623	74000.120574	34.620493
1077.960886	74094.260021	34.625511
1078.987012	74239.672741	34.630528
1080.335454	74333.741637	34.635546
1081.369666	74446.566105	34.640564
1082.444406	74565.893689	34.645581
1083.504236	74688.693698	34.650599
1084.633513	74801.340739	34.655616
1085.150821	74912.878735	34.660634
1086.741065	75024.619542	34.665652
1087.929233	75156.723253	34.670669
1088.990854	75243.549304	34.675687
1090.530180	75383.131568	34.680704
1091.725419	75473.097161	34.685722
1093.317318	75563.322369	34.690740
1094.201174	75678.812976	34.695757
1094.909434	75788.758170	34.700775
1096.062469	75871.742638	34.705792
1097.258528	76010.549642	34.710810
1097.925484	76074.456952	34.715828
1099.419172	76160.510419	34.720845
1099.886529	76294.126602	34.725863
1101.082354	76348.154836	34.730880
1102.009250	76506.555536	34.735898
1102.712215	76581.998964	34.740916
1104.238108	76692.191907	34.745933
1104.998134	76783.060487	34.750951
1106.246798	76920.702483	34.755968
1107.179314	77008.915486	34.760986
1108.004973	77139.275956	34.766004
1109.232503	77215.763299	34.771021
1110.527507	77357.344678	34.776039
1111.488901	77471.000315	34.781056
1112.615736	77602.560944	34.786074
1113.799968	77712.617843	34.791092
1114.828441	77828.401079	34.796109
1115.474095	77946.957311	34.801127
1116.918632	78080.638397	34.806144
1118.206483	78197.374786	34.811162
1119.021852	78313.807756	34.816180
1120.192254	78455.410261	34.821197
1121.463633	78578.016925	34.826215
1122.373893	78681.606090	34.831232
1123.312316	78835.769291	34.836250
1125.094229	78946.199194	34.841268
1126.145092	79074.513581	34.846285
1127.437269	79203.985022	34.851303
1128.946914	79315.800229	34.856320
1130.194131	79422.670625	34.861338
1131.336448	79556.358852	34.866356
1132.621140	79641.063369	34.871373
1133.343051	79793.662680	34.876391
1134.929565	79870.627523	34.881408
1136.271181	80015.487843	34.886426
1137.283554	80120.142603	34.891444
1138.684722	80232.858681	34.896461
1139.144107	80349.170174	34.901479
1140.641756	80470.114974	34.906496
1141.599157	80580.924999	34.911514
1142.463029	80690.808627	34.916532
1143.992684	80810.871680	34.921549
1145.629371	80934.913483	34.926567
1146.685080	81042.574974	34.931584
1147.706623	81151.993481	34.936602
1148.789083	81261.143700	34.941620
1149.689566	81394.066821	34.946637
1150.652395	81506.025117	34.951655
1152.227694	81615.756261	34.956672
1153.161141	81734.591962	34.961690
1154.013871	81868.277975	34.966708
1155.706485	81980.660107	34.971725
1156.578422	82085.890794	34.976743
1157.702789	82237.894117	34.981760
1158.899571	82329.602804	34.986778
1159.747375	82452.287195	34.991796
1160.947862	82548.295067	34.996813
1161.689644	82666.736678	35.001831
1163.033086	82776.548745	35.006848
1164.207110	82878.112951	35.011866
1165.360410	83012.947016	35.016884
1166.833486	83094.405182	35.021901
1167.528641	83248.962325	35.026919
1168.908321	83332.377130	35.031936
1169.821243	83452.863282	35.036954
1170.893703	83604.024981	35.041972
1172.251471	83724.404018	35.046989
1173.101611	83848.019246	35.052007
1174.336130	83959.372161	35.057024
1175.521490	84063.690479	35.062042
1176.839186	84191.741151	35.067060
1178.128874	84343.101220	35.072077
1179.621022	84437.895410	35.077095
1180.724777	84580.075045	35.082112
1181.676698	84694.732833	35.087130
1182.944222	84802.538060	35.092148
1184.117840	84970.486003	35.097165
1185.068659	85085.620276	35.102183
1186.425629	85206.829840	35.107200
1188.054887	85306.537763	35.112218
1188.801528	85482.125855	35.117236
1190.264257	85575.975105	35.122253
1191.272833	85733.402726	35.127271
1192.884578	85828.854351	35.132288
1194.164347	85970.794033	35.137306
1195.058483	86070.616122	35.142324
1196.515052	86222.715507	35.147341
1197.659264	86342.138065	35.152359
1198.690019	86455.553536	35.157376
1200.171632	86598.812103	35.162394
1201.279043	86715.352984	35.167412
1202.493688	86831.302049	35.172429
1204.034932	86976.336780	35.177447
1204.977961	87104.749151	35.182464
1205.569844	87219.047824	35.187482
1207.606280	87324.985734	35.192500
1209.053551	87482.135186	35.197517
1210.423056	87613.796195	35.202535
1211.284152	87698.986343	35.207552
1212.596153	87840.579216	35.212570
1213.713883	87982.437879	35.217588
1215.002477	88073.651001	35.222605
1216.462527	88174.499530	35.227623
1217.547106	88327.096691	35.232640
1218.714291	88463.297426	35.237658
1219.975745	88555.547650	35.242676
1221.291233	88708.066527	35.247693
1222.370120	88823.010860	35.252711
1223.735062	88920.412632	35.257728
1224.892891	89025.771410	35.262746
1226.025635	89184.602175	35.267764
1226.990239	89261.434658	35.272781
1228.640347	89344.570779	35.277799
1229.235983	89495.388403	35.282816
1230.487579	89623.747756	35.287834
1231.140167	89719.805568	35.292852
1232.749480	89812.309398	35.297869
1233.634421	89919.081886	35.302887
1234.753629	90096.077666	35.307904
1236.100982	90216.627754	35.312922
1237.289988	90318.187085	35.317940
1238.783973	90482.345398	35.322957
1239.917250	90597.929228	35.327975
1241.149433	90700.868476	35.332992
1242.447414	90862.341399	35.338010
1243.440705	90977.481500	35.343028
1244.675178	91100.489279	35.348045
1246.140165	91267.934115	35.353063
1246.734929	91383.133388	35.358080
1248.471779	91497.165072	35.363098
1249.488998	91677.484916	35.368116
1250.887307	91784.735137	35.373133
1251.854660	91966.475651	35.378151
1252.913365	92100.053741	35.383168
1254.401595	92220.073857	35.388186
1255.522549	92402.761225	35.393204
1256.901013	92524.115990	35.398221
1258.454990	92673.772220	35.403239
1259.362193	92825.600512	35.408256
1261.368380	92966.338397	35.413274
1262.501047	93101.093543	35.418292
1263.737396	93258.640797	35.423309
1265.317538	93376.204836	35.428327
1266.587650	93551.869904	35.433344
1268.320213	93647.475934	35.438362
1269.159982	93826.797906	35.443380
1270.579564	93929.355613	35.448397
1271.906934	94092.530024	35.453415
1273.293481	94217.371645	35.458432
1274.367521	94365.091530	35.463450
1276.107073	94476.234886	35.468468
1277.199380	94641.443158	35.473485
1278.736078	94745.965847	35.478503
1279.743169	94906.179929	35.483520
1281.447518	95022.556405	35.488538
1282.346725	95162.041992	35.493556
1283.621274	95282.422606	35.498573
1285.113514	95432.170489	35.503591
1286.405104	95545.939593	35.508608
1287.597152	95712.253221	35.513626
1288.961336	95802.006262	35.518644
1290.123832	95977.277381	35.523661
1291.415563	96082.876352	35.528679
1292.373853	96217.659073	35.533696
1293.832620	96371.916182	35.538714
1294.781940	96501.154270	35.543732
1296.208517	96596.650783	35.548749
1297.739187	96732.920742	35.553767
1298.859440	96881.440596	35.558784
1299.919663	96967.596521	35.563802
1301.224670	97071.167369	35.568820
1302.130254	97237.082313	35.573837
1303.708461	97371.925204	35.578855
1305.009521	97472.879509	35.583872
1306.678284	97646.792573	35.588890
1307.470048	97757.685312	35.593908
1309.092543	97896.636328	35.598925
1310.164962	98035.555437	35.603943
1311.342045	98151.323357	35.608960
1312.874761	98269.939135	35.613978
1314.140920	98410.936416	35.618996
1315.562431	98550.309286	35.624013
1316.928408	98729.947254	35.629031
1317.839503	98872.857492	35.634048
1319.477630	98989.568627	35.639066
1320.989418	99128.298018	35.644084
1322.279879	99304.953699	35.649101
1323.991831	99413.171228	35.654119
1325.132372	99557.915640	35.659136
1326.377938	99709.901063	35.664154
1327.950178	99832.612086	35.669172
1328.807372	99994.859922	35.674189
1330.440320	100105.415226	35.679207
1331.947930	100279.127197	35.684224
1333.369388	100371.894484	35.689242
1334.507998	100549.387388	35.694260
1335.670664	100656.432690	35.699277
1337.433204	100835.473642	35.704295
1338.282540	100963.348272	35.709312
1339.790201	101103.735284	35.714330
1341.245267	101263.847009	35.719348
1342.635888	101373.194127	35.724365
1344.572053	101521.253746	35.729383
1345.399293	101691.345063	35.734400
1347.258870	101831.813422	35.739418
1348.380714	101973.678023	35.744436
1349.414104	102071.449168	35.749453
1351.147713	102208.649577	35.754471
1352.351294	102393.112774	35.759488
1353.404573	102507.188539	35.764506
1355.500132	102621.213092	35.769524
1356.646810	102780.618641	35.774541
1358.045573	102947.787190	35.779559
1359.233493	103076.290343	35.784576
1360.414037	103220.317254	35.789594
1362.021429	103355.994178	35.794612
1362.779665	103523.812828	35.799629
1364.301742	103636.629960	35.804647
1365.736338	103781.189438	35.809664
1366.875284	103944.419827	35.814682
1368.304878	104044.642096	35.819700
1369.600674	104207.805086	35.824717
1370.967621	104355.979466	35.829735
1372.207680	104487.335984	35.834752
1373.420512	104595.625353	35.839770
1374.812960	104715.125403	35.844788
1375.597699	104889.315641	35.849805
1377.569454	105008.364395	35.854823
1378.563957	105176.562246	35.859840
1379.508050	105320.930668	35.864858
1381.479583	105439.171604	35.869876
1382.621747	105631.782825	35.874893
1384.322179	105742.006029	35.879911
1385.471842	105928.245769	35.884928
1387.237625	106030.460779	35.889946
1388.642087	106219.231655	35.894964
1390.329742	106343.369758	35.899981
1391.893354	106490.906015	35.904999
1392.931230	106669.676259	35.910016
1394.250369	106779.933222	35.915034
1395.953263	106957.821501	35.920052
1397.087628	107081.405843	35.925069
1398.735476	107266.032613	35.930087
1399.976650	107402.316180	35.935104
1401.603929	107550.101994	35.940122
1402.897420	107717.922127	35.945140
1404.134792	107843.943310	35.950157
1405.670277	108022.606563	35.955175
1407.180183	108144.763296	35.960192
1408.603872	108302.282146	35.965210
1410.162113	108473.780623	35.970228
1411.383060	108607.472954	35.975245
1412.804630	108773.229424	35.980263
1414.264017	108929.980854	35.985280
1415.966798	109068.858746	35.990298
1417.737666	109228.999400	35.995316
1418.917202	109382.848773	36.000333
1420.378975	109536.097280	36.005351
1422.384778	109666.512354	36.010368
1423.358200	109845.569518	36.015386
1424.787424	109953.525883	36.020404
1426.099287	110137.829192	36.025421
1427.652644	110258.274355	36.030439
1428.537505	110445.945550	36.035456
1430.062461	110567.384170	36.040474
1431.729142	110719.822667	36.045492
1432.817839	110931.676264	36.050509
1434.431283	111057.141627	36.055527
1435.481394	111198.141893	36.060544
1437.208522	111374.229373	36.065562
1438.866921	111499.132821	36.070580
1440.338314	111696.348120	36.075597
1442.064952	111820.052323	36.080615
1443.126485	111987.793112	36.085632
1445.121962	112146.170063	36.090650
1446.718447	112252.388186	36.095668
1447.566885	112423.666328	36.100685
1448.983514	112523.894246	36.105703
1450.299471	112685.066611	36.110720
1451.306544	112793.064546	36.115738
1452.660247	112970.127953	36.120756
1454.598860	113089.234366	36.125773
1455.771385	113254.256713	36.130791
1457.288968	113374.374616	36.135808
1458.682694	113558.373932	36.140826
1460.377550	113678.617062	36.145844
1461.667288	113853.702820	36.150861
1463.096018	113971.742326	36.155879
1464.433104	114159.945874	36.160896
1465.670928	114288.703211	36.165914
1467.096482	114467.962538	36.170932
1468.626851	114602.347258	36.175949
1469.895667	114762.837816	36.180967
1471.551945	114969.621695	36.185984
1472.505180	115101.264601	36.191002
1474.506578	115276.152233	36.196020
1475.807558	115487.681643	36.201037
1477.386025	115623.032795	36.206055
1478.995014	115772.225655	36.211072
1480.660839	115983.308716	36.216090
1481.871290	116116.023965	36.221108
1483.482528	116308.334163	36.226125
1485.122219	116453.233664	36.231143
1486.984518	116626.810529	36.236160
1488.124828	116802.738218	36.241178
1490.294670	116979.757131	36.246196
1491.538293	117115.606305	36.251213
1492.827484	117306.892561	36.256231
1494.868442	117436.582976	36.261248
1496.183492	117630.849629	36.266266
1497.555212	117775.191401	36.271284
1498.768236	117978.568888	36.276301
1500.385909	118105.740358	36.281319
1501.957862	118284.876732	36.286336
1503.396985	118484.480324	36.291354
1505.447021	118618.018585	36.296372
1506.571817	118787.377414	36.301389
1508.568322	118943.270506	36.306407
1509.785020	119117.720295	36.311424
1511.788995	119289.621082	36.316442
1513.203579	119434.927785	36.321460
1514.641435	119621.173774	36.326477
1516.662806	119763.739172	36.331495
1517.786534	119924.348513	36.336512
1519.048102	120099.082713	36.341530
1521.100967	120232.438901	36.346548
1522.332542	120396.928247	36.351565
1523.798948	120547.513917	36.356583
1525.464959	120729.527044	36.361600
1526.808399	120857.135533	36.366618
1528.625905	121021.497729	36.371636
1529.831987	121161.553424	36.376653
1531.481719	121294.029244	36.381671
1532.811645	121424.251564	36.386688
1533.566682	121588.735455	36.391706
1535.712502	121730.265981	36.396724
1536.629055	121873.043755	36.401741
1538.287436	122032.814867	36.406759
1539.437420	122207.219901	36.411776
1540.777153	122362.357550	36.416794
1542.559308	122516.792560	36.421812
1543.983713	122690.498595	36.426829
1545.364057	122872.141312	36.431847
1546.595434	123025.539571	36.436864
1548.188511	123236.142286	36.441882
1549.683868	123390.412636	36.446900
1551.595933	123567.504662	36.451917
1553.290178	123759.970786	36.456935
1554.907229	123938.720708	36.461952
1556.502252	124103.796050	36.466970
1558.421997	124294.811616	36.471988
1559.702242	124459.863166	36.477005
1561.278348	124638.826930	36.482023
1563.281620	124782.081001	36.487040
1564.540855	124999.489130	36.492058
1566.102986	125162.549592	36.497076
1567.966308	125324.663870	36.502093
1569.537445	125530.525497	36.507111
1571.130550	125673.393475	36.512128
1572.778036	125871.442868	36.517146
1574.458666	126037.897173	36.522164
1575.774260	126212.846700	36.527181
1577.575593	126388.556220	36.532199
1579.157132	126580.705754	36.537216
1580.685100	126733.229378	36.542234
1582.405302	126919.203006	36.547252
1584.188030	127096.604812	36.552269
1586.117619	127257.250712	36.557287
1587.340564	127477.344645	36.562304
1588.968098	127629.122746	36.567322
1591.344471	127774.740241	36.572340
1592.061519	127978.159186	36.577357
1593.971928	128123.434516	36.582375
1595.579339	128318.847807	36.587392
1597.321371	128490.653207	36.592410
1598.915185	128646.622747	36.597428
1600.138573	128851.373873	36.602445
1601.703052	128994.213116	36.607463
1603.320657	129194.166232	36.612480
1604.893759	129350.649773	36.617498
1606.735609	129521.394254	36.622516
1607.954905	129744.864031	36.627533
1609.469064	129894.062883	36.632551
1611.590460	130074.571922	36.637568
1613.104051	130225.939003	36.642586
1614.622345	130407.394809	36.647604
1616.369853	130535.364954	36.652621
1618.022784	130731.054072	36.657639
1619.307483	130866.143242	36.662656
1620.859543	131021.968060	36.667674
1622.633453	131213.574526	36.672692
1623.834811	131357.864531	36.677709
1625.626175	131490.241010	36.682727
1627.069117	131708.623200	36.687744
1628.311069	131872.053013	36.692762
1629.742915	132030.436432	36.697780
1631.771740	132191.804661	36.702797
1633.210144	132409.736887	36.707815
1635.008681	132581.659866	36.712832
1636.544883	132754.373084	36.717850
1638.352244	132925.397180	36.722868
1639.682895	133142.439906	36.727885
1641.628808	133300.736110	36.732903
1643.043824	133505.313390	36.737920
1644.735126	133658.292484	36.742938
1646.282556	133871.213799	36.747956
1647.753122	134079.118697	36.752973
1649.738201	134254.519223	36.757991
1651.050812	134434.614424	36.763008
1652.788543	134625.286700	36.768026
1654.802974	134859.871604	36.773044
1656.276602	135035.396141	36.778061
1658.022582	135217.404084	36.783079
1660.392136	135412.530135	36.788096
1661.455143	135629.988975	36.793114
1663.413557	135788.461646	36.798132
1665.337247	135984.093188	36.803149
1666.928848	136196.834599	36.808167
1668.734580	136356.741158	36.813184
1670.427170	136579.606571	36.818202
1671.761937	136754.377926	36.823220
1673.807438	136938.021759	36.828237
1675.287731	137147.822582	36.833255
1676.685846	137323.423622	36.838272
1678.706486	137496.493817	36.843290
1680.235537	137685.217141	36.848308
1682.075276	137924.112331	36.853325
1683.878634	138130.738828	36.858343
1685.627267	138302.501028	36.863360
1687.045177	138488.598618	36.868378
1689.434615	138677.381743	36.873396
1690.999023	138867.931865	36.878413
1692.631093	139066.380240	36.883431
1694.726130	139245.569805	36.888448
1696.361318	139420.144517	36.893466
1698.282520	139611.643905	36.898484
1700.223574	139774.969241	36.903501
1701.572296	140003.516597	36.908519
1703.136829	140155.041772	36.913536
1704.237175	140332.646932	36.918554
1706.234899	140485.917267	36.923572
1707.526901	140670.882538	36.928589
1709.163537	140850.344627	36.933607
1711.501915	141034.639034	36.938624
1713.002952	141208.130201	36.943642
1714.303845	141343.759829	36.948660
1716.361993	141496.277973	36.953677
1717.832833	141669.713219	36.958695
1719.831086	141852.900645	36.963712
1721.427473	142030.943994	36.968730
1722.473448	142223.574893	36.973748
1724.314866	142408.172046	36.978765
1725.350403	142601.149192	36.983783
1727.899356	142766.460105	36.988800
1729.685661	142971.411632	36.993818
1731.444898	143201.286789	36.998836
1733.241204	143364.489751	37.003853
1735.007102	143547.749610	37.008871
1736.525205	143745.448337	37.013888
1738.492295	143941.568744	37.018906
1740.077956	144128.168793	37.023924
1741.805377	144305.976426	37.028941
1743.194325	144530.127877	37.033959
1745.581771	144690.670982	37.038976
1747.127838	144915.066447	37.043994
1749.165557	145130.373369	37.049012
1750.917604	145310.768608	37.054029
1752.410806	145501.827969	37.059047
1754.236283	145688.919021	37.064064
1755.882731	145881.756292	37.069082
1758.135166	146110.104378	37.074100
1759.664483	146304.902227	37.079117
1761.203698	146473.562235	37.084135
1763.363021	146717.799616	37.089152
1765.039018	146885.907731	37.094170
1767.014546	147111.505679	37.099188
1769.028344	147289.715823	37.104205
1770.574506	147477.812588	37.109223
1772.714459	147700.143528	37.114240
1774.455092	147872.277684	37.119258
1776.157268	148101.475463	37.124276
1778.094172	148263.616900	37.129293
1779.654437	148480.784591	37.134311
1781.496595	148659.967747	37.139328
1783.425236	148836.615509	37.144346
1785.008536	149061.186695	37.149364
1787.122291	149240.431395	37.154381
1788.858315	149438.473616	37.159399
1790.813947	149653.837065	37.164416
1792.307144	149844.402848	37.169434
1794.567125	150025.086576	37.174452
1795.952657	150233.622660	37.179469
1797.894626	150410.276949	37.184487
1799.640918	150628.367727	37.189504
1801.633942	150778.646875	37.194522
1803.695014	150986.002959	37.199540
1805.275982	151127.614298	37.204557
1806.926063	151302.950600	37.209575
1808.247671	151491.245954	37.214592
1809.988715	151644.890680	37.219610
1811.439059	151856.051174	37.224628
1813.231235	152009.879664	37.229645
1814.826299	152234.597721	37.234663
1817.031914	152398.327344	37.239680
1818.731675	152606.638522	37.244698
1820.316090	152763.799852	37.249716
1822.017167	153001.222593	37.254733
1823.602419	153204.978838	37.259751
1825.749624	153367.429342	37.264768
1827.327923	153604.761789	37.269786
1829.375717	153787.566572	37.274804
1831.263897	153975.114179	37.279821
1833.128673	154214.307295	37.284839
1834.854894	154385.971023	37.289856
1836.832481	154626.290273	37.294874
1838.561020	154794.519728	37.299892
1840.804050	155031.325686	37.304909
1842.434973	155222.128929	37.309927
1844.650464	155401.429125	37.314944
1846.498237	155651.792914	37.319962
1848.523953	155861.074305	37.324980
1850.045870	156029.685065	37.329997
1852.163721	156238.535737	37.335015
1854.160698	156461.696841	37.340032
1855.907721	156692.316727	37.345050
1858.017244	156885.995053	37.350068
1859.736178	157088.472916	37.355085
1861.276962	157288.317463	37.360103
1864.153914	157453.841817	37.365120
1866.089402	157706.501849	37.370138
1867.844803	157919.718877	37.375156
1869.894445	158111.283353	37.380173
1871.341627	158294.169737	37.385191
1873.459801	158472.030588	37.390208
1875.584998	158662.901386	37.395226
1877.348105	158913.086864	37.400244
1879.023689	159092.847149	37.405261
1881.258406	159276.907126	37.410279
1882.912801	159503.134936	37.415296
1884.659922	159678.955849	37.420314
1886.742066	159905.536831	37.425332
1888.962853	160089.793512	37.430349
1890.706446	160308.353051	37.435367
1892.872792	160468.995568	37.440384
1894.363837	160698.871123	37.445402
1896.491284	160875.690192	37.450420
1898.189862	161079.386538	37.455437
1900.198256	161296.933698	37.460455
1902.281778	161480.826304	37.465472
1904.294396	161662.258217	37.470490
1905.814890	161856.425404	37.475508
1907.946294	161990.271462	37.480525
1909.653069	162182.407155	37.485543
1910.969776	162362.431274	37.490560
1912.890148	162517.985980	37.495578
1914.672966	162727.321783	37.500596
1916.818043	162876.082919	37.505613
1918.242101	163106.022654	37.510631
1920.471669	163274.086785	37.515648
1922.164046	163489.541460	37.520666
1924.041719	163651.030415	37.525684
1925.816068	163891.458482	37.530701
1927.274373	164079.610737	37.535719
1929.036016	164266.675860	37.540736
1931.725130	164456.930245	37.545754
1933.584916	164665.618217	37.550772
1935.443432	164916.033557	37.555789
1937.025402	165122.016078	37.560807
1939.446576	165306.572121	37.565824
1941.343313	165542.704823	37.570842
1942.526249	165742.019524	37.575860
1945.365280	165936.075356	37.580877
1947.113570	166186.009492	37.585895
1948.997890	166372.786827	37.590912
1951.457980	166586.958311	37.595930
1953.104883	166819.765049	37.600948
1955.797244	167002.764510	37.605965
1957.521106	167225.934875	37.610983
1959.493753	167440.683268	37.616000
1962.272442	167624.204779	37.621018
1963.806764	167832.683176	37.626036
1965.979802	168083.881684	37.631053
1967.667724	168277.206447	37.636071
1969.942821	168459.010841	37.641088
1971.790998	168706.041302	37.646106
1973.713001	168904.025178	37.651124
1976.072668	169075.316734	37.656141
1978.164064	169272.793652	37.661159
1979.861204	169531.954113	37.666176
1981.863868	169725.997341	37.671194
1983.866312	169924.772853	37.676212
1986.234058	170123.263105	37.681229
1987.683289	170314.441657	37.686247
1990.276455	170520.800625	37.691264
1992.553063	170744.436656	37.696282
1994.102522	170921.852169	37.701300
1996.529477	171094.943281	37.706317
1998.025213	171331.454779	37.711335
1999.910123	171553.305640	37.716352
2002.176258	171733.401804	37.721370
2004.294548	171928.706222	37.726388
2006.241708	172166.406954	37.731405
2007.949564	172337.816404	37.736423
2009.891956	172549.883537	37.741440
2011.689682	172756.773799	37.746458
2013.959732	172918.202048	37.751476
2015.825558	173138.872465	37.756493
2017.978145	173311.154293	37.761511
2019.989315	173490.119204	37.766528
2021.675539	173675.935950	37.771546
2023.815141	173833.849351	37.776564
2026.141186	173998.419147	37.781581
2027.651763	174224.809764	37.786599
2029.640256	174433.391053	37.791616
2031.997806	174605.722068	37.796634
2033.574804	174838.524653	37.801652
2035.425382	175016.215218	37.806669
2037.783524	175200.245176	37.811687
2039.515463	175443.378483	37.816704
2041.462631	175610.399984	37.821722
2043.663754	175822.341921	37.826740
2046.063192	176021.757478	37.831757
2048.222253	176236.613410	37.836775
2049.951860	176415.724793	37.841792
2052.150002	176664.119712	37.846810
2054.154184	176857.601338	37.851828
2056.713625	177041.239760	37.856845
2058.406619	177282.842410	37.861863
2060.462073	177472.170236	37.866880
2063.429617	177657.053388	37.871898
2064.996729	177891.143591	37.876916
2067.333232	178073.337604	37.881933
2068.990116	178307.060666	37.886951
2071.464801	178472.170474	37.891968
2073.594081	178699.845179	37.896986
2076.229264	178914.842472	37.902004
2078.194682	179096.731892	37.907021
2080.205897	179326.204938	37.912039
2082.179131	179495.724707	37.917056
2084.998721	179674.778699	37.922074
2086.308036	179877.557577	37.927092
2088.570668	180083.941695	37.932109
2090.778712	180325.822724	37.937127
2092.921710	180507.081023	37.942144
2095.124939	180687.949906	37.947162
2097.503411	180875.186393	37.952180
2099.377522	181102.609976	37.957197
2101.703533	181314.712201	37.962215
2103.636711	181487.570474	37.967232
2106.570516	181657.263644	37.972250
2108.353521	181871.142253	37.977268
2110.160728	182088.202798	37.982285
2112.499112	182247.017503	37.987303
2114.353164	182459.136767	37.992320
2116.691187	182620.477853	37.997338
2118.514544	182855.557032	38.002356
2120.515461	183023.221131	38.007373
2122.810327	183209.681600	38.012391
2124.927614	183398.975190	38.017408
2127.263654	183612.761902	38.022426
2129.365021	183797.669484	38.027444
2131.520703	183920.242468	38.032461
2133.426582	184128.922939	38.037479
2135.548572	184256.603066	38.042496
2137.357290	184448.944646	38.047514
2138.590923	184649.638732	38.052532
2140.733964	184803.418102	38.057549
2142.896345	184990.795305	38.062567
2144.751464	185187.662662	38.067584
2146.827092	185385.244559	38.072602
2148.467105	185580.180947	38.077620
2150.714602	185806.186469	38.082637
2152.857324	185994.357696	38.087655
2155.046587	186207.900930	38.092672
2157.400519	186430.885317	38.097690
2159.181457	186631.564841	38.102708
2162.052611	186820.283794	38.107725
2164.513311	187077.109938	38.112743
2166.348505	187263.571335	38.117760
2168.626325	187487.055144	38.122778
2170.668823	187694.347210	38.127796
2173.014213	187908.926852	38.132813
2175.221416	188136.270003	38.137831
2177.753159	188319.452719	38.142848
2179.879343	188565.109637	38.147866
2181.913714	188753.245890	38.152884
2184.663734	188989.948472	38.157901
2186.830543	189191.034730	38.162919
2189.019723	189411.813460	38.167936
2191.308274	189612.806070	38.172954
2193.366770	189810.105077	38.177972
2196.312567	190028.799693	38.182989
2198.708310	190249.968354	38.188007
2200.809083	190408.290922	38.193024
2203.252384	190655.888136	38.198042
2205.230868	190834.637864	38.203060
2207.924141	191023.605050	38.208077
2209.653358	191239.604706	38.213095
2211.934134	191416.823850	38.218112
2214.261975	191651.043112	38.223130
2216.288249	191854.764499	38.228148
2218.462926	192037.891291	38.233165
2221.204226	192228.594229	38.238183
2223.484667	192427.797812	38.243200
2225.701940	192615.679139	38.248218
2227.336692	192879.292431	38.253236
2229.537566	193066.594295	38.258253
2231.991137	193242.802771	38.263271
2234.003122	193481.053236	38.268288
2236.365972	193651.008081	38.273306
2238.366963	193900.417950	38.278324
2240.390789	194077.294043	38.283341
2242.942228	194311.642828	38.288359
2244.878197	194517.128278	38.293376
2247.329735	194688.760572	38.298394
2249.098652	194925.140054	38.303412
2251.392491	195095.453434	38.308429
2253.452109	195276.947846	38.313447
2255.323592	195495.063065	38.318464
2257.712747	195664.360598	38.323482
2259.407059	195900.654928	38.328500
2261.453407	196083.144290	38.333517
2263.885752	196302.392446	38.338535
2265.821952	196518.597983	38.343552
2267.618242	196737.568101	38.348570
2270.260134	196965.860684	38.353588
2272.305233	197180.401750	38.358605
2275.089794	197415.654390	38.363623
2276.884291	197674.913902	38.368640
2278.828882	197879.954573	38.373658
2281.910930	198095.096518	38.378676
2284.197374	198316.737114	38.383693
2286.329794	198550.676716	38.388711
2288.381285	198834.410428	38.393728
2290.682630	199081.614715	38.398746
2293.105238	199303.999415	38.403764
2295.523955	199518.643092	38.408781
2297.780981	199801.422795	38.413799
2300.150963	200017.777036	38.418816
2302.498893	200250.788735	38.423834
2304.810291	200504.331753	38.428852
2307.418009	200740.084128	38.433869
2309.709946	201007.049104	38.438887
2311.555794	201282.717457	38.443904
2314.264180	201506.957197	38.448922
2316.911887	201750.323512	38.453940
2318.665456	201994.632353	38.458957
2321.748160	202228.906867	38.463975
2324.442967	202468.435484	38.468992
2326.876502	202718.846785	38.474010
2329.090690	203004.455081	38.479028
2331.349536	203246.759884	38.484045
2333.831669	203476.704798	38.489063
2335.682230	203707.766280	38.494080
2338.737459	203929.447435	38.499098
2340.839192	204209.405553	38.504116
2343.126537	204481.757376	38.509133
2346.025198	204672.962891	38.514151
2348.039370	204894.457425	38.519168
2350.717476	205138.937955	38.524186
2352.796203	205379.274731	38.529204
2354.857555	205655.336518	38.534221
2357.069237	205919.316305	38.539239
2359.648731	206163.296321	38.544256
2361.943397	206397.649463	38.549274
2364.215502	206663.755662	38.554292
2366.387172	206890.754852	38.559309
2369.042918	207133.546221	38.564327
2371.272724	207394.127629	38.569344
2373.638091	207639.480608	38.574362
2376.134941	207866.444660	38.579380
2378.801145	208089.333130	38.584397
2380.960166	208319.043712	38.589415
2382.743531	208552.610448	38.594432
2385.027497	208744.586765	38.599450
2387.311682	208950.007474	38.604468
2389.410696	209222.855323	38.609485
2391.739461	209449.369539	38.614503
2394.424359	209661.876357	38.619520
2396.364269	209918.502949	38.624538
2398.082525	210183.100165	38.629556
2401.172736	210406.996251	38.634573
2403.416084	210674.724179	38.639591
2405.716671	210974.867808	38.644608
2408.205096	211221.777113	38.649626
2410.208095	211465.438154	38.654644
2412.863897	211720.117807	38.659661
2415.591265	212009.851944	38.664679
2417.710211	212275.041873	38.669696
2420.380359	212506.349976	38.674714
2422.794021	212805.240130	38.679732
2425.267581	213107.600778	38.684749
2427.754685	213370.807096	38.689767
2430.302341	213606.569339	38.694784
2433.260827	213864.091396	38.699802
2435.462993	214145.818386	38.704820
2437.220752	214432.454159	38.709837
2439.768856	214695.262518	38.714855
2442.772459	214988.901816	38.719872
2444.846106	215265.423141	38.724890
2447.993394	215539.858307	38.729908
2450.361343	215811.523386	38.734925
2452.981220	216081.359449	38.739943
2455.604217	216345.927130	38.744960
2458.169033	216624.509095	38.749978
2460.821620	216931.721299	38.754996
2462.658479	217204.466376	38.760013
2466.159137	217430.657462	38.765031
2468.177892	217749.768753	38.770048
2470.549044	217996.569406	38.775066
2473.426946	218267.185639	38.780084
2475.914353	218576.894365	38.785101
2478.321430	218796.927518	38.790119
2480.522571	219066.435161	38.795136
2482.964029	219344.920458	38.800154
2485.726944	219614.887073	38.805172
2488.162122	219883.700429	38.810189
2490.950794	220157.232802	38.815207
2493.526819	220459.837937	38.820224
2495.935735	220744.961559	38.825242
2498.402057	221036.755853	38.830260
2500.800045	221293.035496	38.835277
2503.403343	221534.034155	38.840295
2505.715821	221821.437263	38.845312
2507.660225	222131.894573	38.850330
2510.275158	222390.416369	38.855348
2512.369829	222646.139186	38.860365
2515.006178	222889.828745	38.865383
2517.429578	223149.259568	38.870400
2519.625356	223396.106022	38.875418
2522.090182	223655.925591	38.880436
2523.827912	223928.609616	38.885453
2526.421469	224200.676446	38.890471
2528.854609	224478.128047	38.895488
2531.202019	224755.124385	38.900506
2534.216726	225043.304236	38.905524
2536.565535	225323.946569	38.910541
2538.993515	225607.015312	38.915559
2541.721028	225900.627611	38.920576
2543.978966	226187.483886	38.925594
2546.428351	226480.774090	38.930612
2548.701783	226779.858116	38.935629
2551.958271	227083.663492	38.940647
2554.248233	227388.435807	38.945664
2556.790380	227691.899441	38.950682
2559.659161	227989.877567	38.955700
2562.080895	228305.552741	38.960717
2564.926605	228608.082643	38.965735
2567.187042	228924.242772	38.970752
2570.321022	229224.621214	38.975770
2573.415266	229527.267302	38.980788
2575.401256	229828.769393	38.985805
2578.431376	230131.376908	38.990823
2580.992231	230445.310724	38.995840
2583.554867	230753.505581	39.000858
2586.522589	231053.560960	39.005876
2588.825473	231353.443296	39.010893
2591.656913	231655.401642	39.015911
2594.380324	231966.927561	39.020928
2597.136774	232265.318715	39.025946
2599.743128	232572.699986	39.030964
2602.291384	232876.408782	39.035981
2604.957709	233179.871255	39.040999
2607.839243	233488.888136	39.046016
2610.065783	233793.895302	39.051034
2613.140239	234087.390731	39.056052
2615.522702	234404.185209	39.061069
2618.250864	234684.936604	39.066087
2621.181163	235004.820981	39.071104
2623.313646	235315.943337	39.076122
2626.262847	235615.482535	39.081140
2628.850075	235901.542535	39.086157
2631.626501	236203.269706	39.091175
2634.184221	236519.839850	39.096192
2636.786036	236816.516725	39.101210
2639.634874	237114.958620	39.106228
2642.160067	237430.469908	39.111245
2645.019884	237724.949544	39.116263
2647.429835	238032.861164	39.121280
2649.984144	238325.104921	39.126298
2652.278811	238600.474729	39.131316
2654.451762	238885.440026	39.136333
2657.169684	239153.606965	39.141351
2659.683613	239438.621256	39.146368
2662.064169	239724.038388	39.151386
2664.730076	240003.797740	39.156404
2667.142962	240306.584473	39.161421
2669.545590	240607.494050	39.166439
2672.195944	240907.933365	39.171456
2674.762893	241225.506107	39.176474
2677.422203	241534.403723	39.181492
2679.955212	241839.842355	39.186509
2682.564676	242158.833233	39.191527
2685.135159	242489.489736	39.196544
2687.704198	242818.039147	39.201562
2690.268814	243143.999307	39.206580
2692.928350	243480.537175	39.211597
2695.858978	243810.022508	39.216615
2698.400371	244143.304198	39.221632
2701.191191	244495.495960	39.226650
2704.027193	244834.930456	39.231668
2706.946120	245182.531668	39.236685
2709.698814	245525.918207	39.241703
2712.878782	245861.236715	39.246720
2715.080009	246208.674833	39.251738
2718.090823	246543.666182	39.256756
2720.809512	246892.700489	39.261773
2723.660086	247245.093088	39.266791
2726.555225	247592.551695	39.271808
2729.085289	247941.440615	39.276826
2731.755564	248287.945845	39.281844
2734.526038	248643.961451	39.286861
2737.620143	248994.693977	39.291879
2740.482992	249342.187167	39.296896
2743.220890	249692.850693	39.301914
2746.012611	250040.178889	39.306932
2748.998948	250394.614827	39.311949
2751.558241	250746.782239	39.316967
2754.706265	251100.203443	39.321984
2757.409104	251450.698515	39.327002
2760.517738	251792.137848	39.332020
2763.060825	252152.337705	39.337037
2765.635435	252493.608986	39.342055
2768.963649	252833.339069	39.347072
2771.452405	253190.476024	39.352090
2774.218099	253536.926410	39.357108
2776.829180	253897.677841	39.362125
2779.740390	254242.633176	39.367143
2782.717785	254581.812384	39.372160
2785.560311	254936.635840	39.377178
2788.330960	255288.550069	39.382196
2790.877991	255642.380091	39.387213
2793.634369	255993.586541	39.392231
2796.923044	256338.053886	39.397248
2799.222895	256676.505623	39.402266
2802.145446	257006.933739	39.407284
2804.909008	257320.113899	39.412301
2807.291504	257632.364151	39.417319
2809.860790	257955.559117	39.422336
2812.195402	258287.352341	39.427354
2815.143989	258601.292427	39.432372
2817.492921	258955.311533	39.437389
2819.923011	259293.365457	39.442407
2823.019470	259639.925808	39.447424
2825.511423	259998.851849	39.452442
2828.041813	260356.527561	39.457460
2831.013422	260716.191502	39.462477
2833.858492	261086.316495	39.467495
2836.824565	261458.328023	39.472512
2839.100113	261826.588142	39.477530
2842.233120	262201.038254	39.482548
2845.257141	262592.500627	39.487565
2847.809454	262972.606860	39.492583
2850.599871	263336.671966	39.497600
2853.619052	263740.152093	39.502618
2856.632142	264122.320521	39.507636
2859.358140	264516.728280	39.512653
2862.120341	264908.920659	39.517671
2865.202239	265304.746267	39.522688
2867.838820	265706.053646	39.527706
2871.030561	266098.941277	39.532724
2874.089766	266498.201045	39.537741
2877.182395	266900.732885	39.542759
2880.284851	267285.989329	39.547776
2883.130552	267693.133506	39.552794
2886.160771	268089.833454	39.557812
2889.159461	268489.993527	39.562829
2892.253623	268878.250022	39.567847
2895.521976	269280.501807	39.572864
2898.141629	269674.016195	39.577882
2901.539947	270061.666369	39.582900
2904.214259	270465.791128	39.587917
2906.860732	270857.117206	39.592935
2910.176866	271253.875370	39.597952
2913.135069	271657.422263	39.602970
2916.233258	272048.601104	39.607988
2919.180384	272438.483017	39.613005
2922.091175	272832.206711	39.618023
2925.144255	273221.970454	39.623040
2927.719074	273634.292018	39.628058
2930.761170	274019.002383	39.633076
2933.858839	274419.758965	39.638093
2936.696253	274821.903174	39.643111
2939.808494	275208.939675	39.648128
2942.700042	275616.892739	39.653146
2946.013657	276012.001063	39.658164
2948.700638	276405.887593	39.663181
2951.620337	276796.536418	39.668199
2954.721026	277187.232755	39.673216
2956.874173	277583.362941	39.678234
2959.897054	277948.795072	39.683252
2962.978126	278310.051756	39.688269
2965.781219	278681.310486	39.693287
2968.312274	279035.388681	39.698304
2971.135734	279415.408132	39.703322
2974.114018	279788.823466	39.708340
2976.642260	280169.956304	39.713357
2979.716697	280566.295327	39.718375
2982.336505	280939.716112	39.723392
2985.108699	281341.538899	39.728410
2988.078676	281729.917206	39.733428
2990.975109	282137.791243	39.738445
2993.686613	282547.955175	39.743463
2996.594666	282952.194152	39.748480
2999.696403	283379.290481	39.753498
3002.692124	283797.435909	39.758516
3005.674990	284235.168871	39.763533
3008.632012	284653.929357	39.768551
3011.974456	285093.128772	39.773568
3015.017649	285528.717055	39.778586
3017.928826	285944.003307	39.783604
3021.403001	286378.125280	39.788621
3024.322959	286816.652986	39.793639
3027.716486	287246.722219	39.798656
3030.678906	287683.768760	39.803674
3033.769944	288112.690842	39.808692
3036.859524	288555.838205	39.813709
3039.965322	288993.317539	39.818727
3043.283829	289417.426098	39.823744
3046.151300	289864.848972	39.828762
3049.540925	290308.606715	39.833780
3052.834824	290738.432817	39.838797
3055.767921	291173.827709	39.843815
3059.278561	291619.418526	39.848832
3062.621066	292052.410096	39.853850
3065.325872	292485.730454	39.858868
3068.477278	292925.965032	39.863885
3071.472829	293362.514695	39.868903
3074.905977	293797.114495	39.873920
3077.571430	294238.464951	39.878938
3080.904195	294666.271105	39.883956
3084.350270	295106.734176	39.888973
3086.897516	295551.428310	39.893991
3090.422947	295982.808378	39.899008
3093.257506	296427.226492	39.904026
3096.554579	296861.485807	39.909044
3099.684723	297303.162518	39.914061
3102.980227	297743.186299	39.919079
3105.886912	298184.032611	39.924096
3108.553312	298628.091085	39.929114
3111.664675	299072.357448	39.934132
3114.838040	299509.906833	39.939149
3117.946034	299965.779957	39.944167
3121.061493	300403.564798	39.949184
3124.302122	300851.743244	39.954202
3127.445982	301259.268200	39.959220
3130.202702	301663.703611	39.964237
3133.049409	302091.086433	39.969255
3136.377253	302490.323667	39.974272
3139.260074	302895.167701	39.979290
3141.963261	303310.275667	39.984308
3145.048705	303739.902109	39.989325
3147.676295	304175.086306	39.994343
3151.153826	304601.981038	39.999360
3154.039588	305037.985354	40.004378
3156.947415	305487.675735	40.009396
3160.127839	305933.181213	40.014413
3163.401124	306399.854489	40.019431
3166.682689	306844.705902	40.024448
3169.581362	307304.323133	40.029466
3172.746536	307755.235092	40.034484
3176.530058	308216.106042	40.039501
3179.478958	308671.443147	40.044519
3182.712046	309145.859722	40.049536
3185.851997	309602.255324	40.054554
3189.027635	310071.165590	40.059572
3192.132070	310541.482237	40.064589
3195.406018	311037.880836	40.069607
3199.275085	311491.181990	40.074624
3202.092701	311983.203782	40.079642
3205.575664	312451.776318	40.084660
3209.177693	312920.074038	40.089677
3212.088000	313393.660567	40.094695
3215.510309	313892.461245	40.099712
3218.958560	314362.758127	40.104730
3222.094902	314832.264094	40.109748
3225.361292	315319.348509	40.114765
3228.561694	315804.307586	40.119783
3231.881791	316254.805393	40.124800
3235.185775	316771.872193	40.129818
3238.664598	317225.515259	40.134836
3242.262532	317734.682515	40.139853
3245.252027	318206.761060	40.144871
3248.502667	318666.554313	40.149888
3252.019240	319168.310698	40.154906
3255.382428	319650.431109	40.159924
3258.543611	320111.907627	40.164941
3261.766881	320612.432709	40.169959
3264.868780	321096.847163	40.174976
3268.533449	321576.928707	40.179994
3271.648627	322062.808818	40.185012
3274.852905	322523.605770	40.190029
3277.957168	323036.300911	40.195047
3281.514093	323518.318930	40.200064
3284.650016	323975.766596	40.205082
3287.687243	324478.711536	40.210100
3291.232609	324966.107026	40.215117
3294.553974	325464.861523	40.220135
3298.122068	325939.448233	40.225152
3301.112526	326413.971151	40.230170
3304.352770	326869.100612	40.235188
3307.501799	327311.315808	40.240205
3310.881737	327769.668557	40.245223
3313.946427	328206.863849	40.250240
3316.975267	328642.005377	40.255258
3320.268202	329115.194372	40.260276
3323.634258	329559.317769	40.265293
3326.120577	330051.699617	40.270311
3329.471181	330498.130773	40.275328
3333.014367	330973.020668	40.280346
3335.742045	331464.059876	40.285364
3339.415356	331908.399936	40.290381
3342.500052	332438.736007	40.295399
3345.876353	332919.073727	40.300416
3349.320179	333409.605495	40.305434
3352.660344	333899.769348	40.310452
3356.222638	334413.230439	40.315469
3359.695479	334910.450719	40.320487
3363.033494	335404.286159	40.325504
3366.516755	335896.673091	40.330522
3369.728554	336420.661449	40.335540
3373.061822	336944.067877	40.340557
3376.477171	337444.960362	40.345575
3380.147102	337960.231016	40.350592
3383.766614	338477.333731	40.355610
3386.660223	339005.617524	40.360628
3390.391678	339517.285942	40.365645
3393.590027	340044.370382	40.370663
3397.107116	340571.552360	40.375680
3400.573132	341090.232322	40.380698
3403.954305	341629.588670	40.385716
3407.639961	342144.848220	40.390733
3410.470826	342670.445122	40.395751
3414.412951	343217.569464	40.400768
3417.746404	343754.426407	40.405786
3421.270969	344267.535273	40.410804
3424.996090	344824.885456	40.415821
3428.152617	345354.494781	40.420839
3431.693297	345892.619695	40.425856
3435.460222	346439.234116	40.430874
3438.521573	346984.050837	40.435892
3442.579714	347514.386327	40.440909
3445.749791	348043.613300	40.445927
3449.010895	348595.237421	40.450944
3452.764102	349149.596181	40.455962
3456.276538	349675.021716	40.460980
3459.956061	350200.618896	40.465997
3463.550611	350756.484302	40.471015
3467.234487	351291.513751	40.476032
3471.224536	351801.992673	40.481050
3474.502028	352349.895370	40.486068
3477.942294	352859.283361	40.491085
3481.246799	353396.687019	40.496103
3484.736121	353930.679830	40.501120
3488.082432	354421.384840	40.506125
3491.299279	354917.815315	40.511130
3494.606838	355343.708952	40.516135
3496.914320	355723.772102	40.521140
3499.602999	356059.975942	40.526144
3502.479790	356329.245097	40.531149
3504.399545	356594.465218	40.536154
3506.176699	356790.997598	40.541159
3508.171312	356926.496769	40.546164
3509.737895	357035.114211	40.551168
3511.275779	357138.722781	40.556173
3512.295530	357175.511467	40.561178
3513.588948	357179.505871	40.566183
3513.972308	357164.812953	40.571188
3514.373388	357157.929633	40.576192
3515.135894	357091.136457	40.581197
3515.619642	357023.903756	40.586202
3515.905893	356941.484480	40.591207
3516.077130	356854.375423	40.596212
3516.475205	356757.534755	40.601216
3516.275687	356631.676061	40.606221
3516.118730	356523.878327	40.611226
3516.518014	356380.467087	40.616231
3516.065390	356275.158566	40.621236
3516.242382	356125.139811	40.626240
3516.276840	356002.678050	40.631245
3515.942153	355847.853319	40.636250
3515.720191	355733.320394	40.641255
3515.900474	355570.753473	40.646260
3515.391315	355445.882369	40.651264
3515.407256	355276.494863	40.656269
3514.423150	355171.827942	40.661274
3514.852091	355010.568700	40.666279
3514.560846	354900.829205	40.671284
3514.145473	354731.533532	40.676288
3513.929145	354642.496946	40.681293
3513.423009	354483.445233	40.686298
3513.381087	354362.035022	40.691303
3512.787560	354237.734193	40.696308
3512.558241	354143.812588	40.701312
3512.493285	353998.075846	40.706317
3511.730475	353912.890871	40.711322
3511.814615	353766.824519	40.716327
3511.461067	353695.418882	40.721332
3511.314844	353568.220865	40.726336
3511.616686	353479.176712	40.731341
3510.947435	353374.481823	40.736346
3510.925828	353268.920853	40.741351
3510.649781	353180.909184	40.746356
3510.385330	353082.257606	40.751360
3509.883223	353019.832788	40.756365
3509.523129	352930.001612	40.761370
3509.704578	352829.930235	40.766375
3509.670724	352766.871196	40.771380
3509.163117	352688.209915	40.776384
3509.300353	352592.751489	40.781389
3508.764153	352555.526832	40.786394
3508.845507	352460.306050	40.791399
3508.855542	352404.467408	40.796404
3508.784904	352334.134991	40.801408
3508.590989	352257.154073	40.806413
3508.191638	352209.167642	40.811418
3508.473373	352118.444670	40.816423
3508.268449	352090.278432	40.821428
3508.274196	352018.253817	40.826432
3507.898584	351955.095141	40.831437
3507.846583	351912.601657	40.836442
3507.863948	351847.548316	40.841447
3507.187568	351789.603380	40.846452
3507.346520	351729.286700	40.851456
3507.227244	351694.845954	40.856461
3507.219440	351645.244649	40.861466
3507.118776	351598.355711	40.866471
3507.019167	351573.811944	40.871476
3507.166466	351493.976447	40.876480
3506.911847	351479.993589	40.881485
3506.705663	351415.305918	40.886490
3506.999488	351381.868579	40.891495
3506.870408	351350.941318	40.896500
3506.700285	351305.335626	40.901504
3506.538475	351262.884437	40.906509
3506.551450	351218.344094	40.911514
3506.336899	351177.046448	40.916519
3506.575707	351162.069281	40.921524
3506.102617	351125.011801	40.926528
3506.297021	351079.653695	40.931533
3506.141260	351048.832280	40.936538
3506.539869	351022.962420	40.941543
3506.128582	350982.993707	40.946548
3506.265034	350952.355096	40.951552
3506.203029	350913.679994	40.956557
3506.031516	350895.382689	40.961562
3505.985715	350833.417633	40.966567
3506.049072	350828.470221	40.971572
3506.094553	350783.822578	40.976576
3505.904122	350774.028751	40.981581
3505.709026	350726.568617	40.986586
3506.092027	350667.640567	40.991591
3505.517454	350691.731481	40.996596
3505.193839	350636.121901	41.001600
3505.353349	350643.630140	41.006605
3505.368939	350608.989223	41.011610
3505.239617	350592.924813	41.016615
3505.147026	350574.131358	41.021620
3505.445018	350541.303659	41.026624
3505.438078	350533.236885	41.031629
3505.319956	350493.272364	41.036634
3505.127322	350495.008057	41.041639
3505.460806	350458.178918	41.046644
3505.180821	350462.473505	41.051648
3505.682756	350417.397086	41.056653
3504.916311	350421.590427	41.061658
3505.267063	350376.868737	41.066663
3505.158624	350370.115980	41.071668
3505.023405	350355.426780	41.076672
3505.187353	350319.667836	41.081677
3504.852112	350323.258545	41.086682
3505.215812	350292.939948	41.091687
3505.105360	350273.487488	41.096692
3504.722454	350259.830006	41.101696
3504.870263	350250.415277	41.106701
3504.888625	350216.613553	41.111706
3505.092334	350213.858129	41.116711
3504.833676	350207.892629	41.121716
3505.198285	350181.238764	41.126720
3505.238964	350161.507862	41.131725
3504.884943	350151.968845	41.136730
3505.122113	350132.537731	41.141735
3505.285811	350107.239044	41.146740
3504.915175	350086.962317	41.151744
3505.215417	350074.036670	41.156749
3504.848267	350052.257769	41.161754
3504.828511	350040.298941	41.166759
3504.921662	350024.860919	41.171764
3504.909039	349987.602610	41.176768
3504.749055	349992.794501	41.181773
3504.779255	349988.310374	41.186778
3505.019246	349949.485039	41.191783
3504.841375	349932.002849	41.196788
3504.575579	349941.894472	41.201792
3505.047237	349904.254132	41.206797
3504.822359	349906.962082	41.211802
3504.807787	349895.969545	41.216807
3504.576915	349868.697039	41.221812
3504.651896	349869.448752	41.226816
3505.007066	349856.463467	41.231821
3504.955679	349827.533694	41.236826
3504.859189	349797.007613	41.241831
3504.703088	349808.918010	41.246836
3504.203607	349779.728187	41.251840
3504.679728	349792.658488	41.256845
3504.783177	349756.577876	41.261850
3504.686885	349762.294193	41.266855
3504.979376	349754.179966	41.271860
3504.595459	349706.774247	41.276864
3505.000874	349723.507969	41.281869
3504.720885	349684.968262	41.286874
3504.814981	349667.468443	41.291879
3504.654772	349681.822832	41.296884
3504.662622	349632.446273	41.301888
3504.784578	349651.489989	41.306893
3504.544458	349603.577874	41.311898
3504.549811	349605.867673	41.316903
3504.666338	349574.544255	41.321908
3504.645346	349563.196348	41.326912
3504.645210	349570.653620	41.331917
3504.517162	349555.810364	41.336922
3504.382596	349519.970836	41.341927
3504.089703	349537.527649	41.346932
3504.014115	349521.327173	41.351936
3504.634317	349510.005142	41.356941
3504.543411	349516.382367	41.361946
3504.437225	349477.865940	41.366951
3504.394486	349495.688634	41.371956
3504.480171	349474.550549	41.376960
3504.776152	349461.778140	41.381965
3503.970001	349466.919527	41.386970
3504.379614	349441.378046	41.391975
3504.531471	349433.387810	41.396980
3504.583527	349426.660466	41.401984
3504.480041	349405.475908	41.406989
3504.228857	349396.378624	41.411994
3504.500549	349388.903915	41.416999
3504.080633	349393.526124	41.422004
3504.181504	349377.730380	41.427008
3504.261385	349359.087400	41.432013
3504.172621	349394.351575	41.437018
3504.541037	349339.242102	41.442023
3504.407282	349365.809042	41.447028
3504.516828	349348.841157	41.452032
3504.278653	349332.004594	41.457037
3503.897005	349325.269450	41.462042
3503.850014	349303.541442	41.467047
3504.304245	349300.491853	41.472052
3503.855925	349319.167717	41.477056
3504.203500	349294.374065	41.482061
3503.967013	349291.993605	41.487066
3504.019608	349294.530461	41.492071
3504.142208	349293.696668	41.497076
3504.257674	349287.290150	41.502080
3504.453265	349279.191172	41.507085
3504.123019	349261.987373	41.512090
3504.302660	349253.483691	41.517095
3504.342812	349253.451925	41.522100
3504.270546	349242.926504	41.527104
3504.435210	349222.463024	41.532109
3504.165752	349227.825002	41.537114
3504.294461	349210.803142	41.542119
3504.259797	349201.900659	41.547124
3504.080044	349195.464449	41.552128
3504.235774	349185.386548	41.557133
3504.272834	349179.959568	41.562138
3504.213437	349178.289197	41.567143
3504.224790	349160.776847	41.572148
3503.925443	349155.352145	41.577152
3504.373814	349160.549742	41.582157
3503.964258	349140.024304	41.587162
3504.021716	349126.373275	41.592167
3504.318487	349132.561997	41.597172
3504.452609	349122.462050	41.602176
3504.569027	349102.642439	41.607181
3504.204602	349105.092524	41.612186
3504.549052	349079.993853	41.617191
3504.580211	349084.137551	41.622196
3504.075728	349072.611466	41.627200
3504.257484	349050.821744	41.632205
3504.457247	349045.852606	41.637210
3504.023924	349029.835799	41.642215
3504.332616	349034.342848	41.647220
3503.968095	349028.750278	41.652224
3504.104492	349011.421724	41.657229
3504.068238	349024.458660	41.662234
3504.188517	349006.979944	41.667239
3504.051648	348990.381775	41.672244
3503.568601	348995.523028	41.677248
3504.191228	348984.302314	41.682253
3504.274976	348995.080551	41.687258
3504.008964	348969.391150	41.692263
3504.215372	348970.732934	41.697268
3504.091040	348970.421753	41.702272
3504.679630	348949.662089	41.707277
3504.376719	348939.554846	41.712282
3504.577762	348929.495187	41.717287
3504.665763	348918.079014	41.722292
3504.394022	348911.148282	41.727296
3504.212730	348893.182724	41.732301
3504.209446	348885.878677	41.737306
3504.386813	348871.368726	41.742311
3504.496722	348865.192102	41.747316
3504.159395	348852.417869	41.752320
3504.288051	348846.187376	41.757325
3504.172672	348822.230252	41.762330
3504.302353	348840.280414	41.767335
3504.428968	348802.490260	41.772340
3504.086069	348807.609374	41.777344
3504.479762	348804.925651	41.782349
3504.231797	348792.213631	41.787354
3504.171519	348764.786351	41.792359
3504.145926	348770.491594	41.797364
3504.300987	348758.275786	41.802368
3504.564008	348746.297423	41.807373
3504.020368	348749.997535	41.812378
3504.112783	348727.483713	41.817383
3504.309870	348724.678359	41.822388
3503.648369	348705.974207	41.827392
3504.186820	348687.462116	41.832397
3504.143204	348707.244980	41.837402
3504.525108	348688.401316	41.842407
3504.417834	348676.735997	41.847412
3504.514203	348667.761809	41.852416
3504.541549	348641.771361	41.857421
3503.974767	348643.362649	41.862426
3504.387042	348625.125002	41.867431
3504.130933	348619.082572	41.872436
3504.144368	348616.688022	41.877440
3504.315123	348598.335840	41.882445
3504.182092	348600.494848	41.887450
3503.897116	348595.347788	41.892455
3503.796438	348590.069784	41.897460
3503.900414	348577.760206	41.902464
3504.279252	348562.302061	41.907469
3504.105449	348572.052126	41.912474
3504.061806	348547.141829	41.917479
3504.016108	348549.287032	41.922484
3504.114575	348550.365922	41.927488
3504.334311	348538.445262	41.932493
3504.303779	348515.721726	41.937498
3504.258085	348517.230636	41.942503
3504.425092	348496.995584	41.947508
3504.226030	348505.324357	41.952512
3504.374504	348482.928832	41.957517
3503.906506	348475.978170	41.962522
3503.939170	348455.789794	41.967527
3503.824153	348463.418088	41.972532
3503.806486	348462.784621	41.977536
3504.298989	348437.025959	41.982541
3504.083868	348436.296449	41.987546
3504.025256	348429.026542	41.992551
3503.986786	348422.109773	41.997556
3503.663294	348410.427678	42.002560
3503.954765	348405.113112	42.007565
3504.233923	348420.976376	42.012570
3504.069389	348409.752734	42.017575
3504.126014	348391.062202	42.022580
3504.372824	348380.333462	42.027584
3504.406488	348367.449562	42.032589
3504.093972	348361.186955	42.037594
3503.961440	348353.139717	42.042599
3504.096074	348348.562592	42.047604
3504.050194	348337.752857	42.052608
3504.092178	348339.986013	42.057613
3503.656965	348346.366902	42.062618
3503.930711	348316.875901	42.067623
3503.911049	348316.115488	42.072628
3504.202152	348318.920104	42.077632
3503.819161	348314.221195	42.082637
3503.981250	348305.847403	42.087642
3503.821110	348289.227253	42.092647
3503.800628	348284.038349	42.097652
3503.710592	348287.208645	42.102656
3503.962971	348281.900247	42.107661
3503.438386	348290.127804	42.112666
3503.909620	348268.241107	42.117671
3504.071217	348258.722052	42.122676
3504.022386	348266.874398	42.127680
3504.057019	348268.905104	42.132685
3504.046803	348263.281894	42.137690
3504.043638	348229.965945	42.142695
3504.233421	348245.156188	42.147700
3503.999592	348230.558368	42.152704
3504.144475	348218.013177	42.157709
3503.909892	348219.679216	42.162714
3503.753290	348214.079144	42.167719
3503.989226	348222.975484	42.172724
3504.108853	348208.372682	42.177728
3504.312865	348191.923999	42.182733
3504.095879	348194.019940	42.187738
3504.015019	348182.655764	42.192743
3504.129762	348172.304190	42.197748
3504.015413	348179.550638	42.202752
3504.576044	348162.714693	42.207757
3504.199391	348155.342319	42.212762
3504.067955	348139.964730	42.217767
3504.360307	348119.455207	42.222772
3504.019043	348123.988729	42.227776
3504.140184	348117.173950	42.232781
3504.049255	348101.535427	42.237786
3504.009155	348092.048231	42.242791
3504.085564	348095.675811	42.247796
3504.229631	348075.546042	42.252800
3504.260123	348059.277464	42.257805
3503.962379	348065.916623	42.262810
3504.121036	348050.773119	42.267815
3504.004083	348028.572087	42.272820
3504.021467	348030.274653	42.277824
3504.369598	348032.357613	42.282829
3503.831624	348004.165567	42.287834
3504.288368	347992.894525	42.292839
3503.977413	348002.539112	42.297844
3503.610149	347986.613369	42.302848
3503.844952	347980.213286	42.307853
3504.062550	347974.681291	42.312858
3504.005317	347980.442520	42.317863
3503.892529	347975.242729	42.322868
3504.018126	347958.526404	42.327872
3504.102514	347947.543287	42.332877
3503.873254	347954.375247	42.337882
3503.786204	347948.611441	42.342887
3504.110110	347920.613970	42.347892
3504.063147	347917.745351	42.352896
3504.235637	347908.733555	42.357901
3503.935734	347917.383781	42.362906
3503.840050	347893.830378	42.367911
3503.788961	347885.872006	42.372916
3503.722937	347890.463841	42.377920
3503.692748	347889.272402	42.382925
3503.545701	347898.178438	42.387930
3503.524197	347886.346682	42.392935
3503.768317	347874.651094	42.397940
3503.781156	347876.939780	42.402944
3504.090930	347873.505720	42.407949
3504.156462	347876.600540	42.412954
3503.949998	347867.165060	42.417959
3503.957971	347850.365490	42.422964
3503.973611	347844.000041	42.427968
3504.265595	347841.688682	42.432973
3503.891773	347823.727766	42.437978
3504.041766	347831.161536	42.442983
3504.205891	347808.992337	42.447988
3503.952362	347805.341904	42.452992
3504.243140	347791.628210	42.457997
3504.262284	347798.853602	42.463002
3503.694686	347793.496629	42.468007
3504.064734	347776.232562	42.473012
3503.942301	347768.005479	42.478016
3504.251403	347770.629113	42.483021
3504.091047	347771.978006	42.488026
3504.095456	347740.416762	42.493031
3504.008384	347727.755420	42.498036
3504.097017	347741.841899	42.503040
3504.061088	347717.846289	42.508045
3503.769938	347713.234618	42.513050
3503.865277	347701.409803	42.518055
3504.109030	347715.471765	42.523060
3504.047737	347690.843851	42.528064
3503.896479	347689.747905	42.533069
3503.809084	347683.246015	42.538074
3503.811928	347667.287121	42.543079
3503.964291	347686.250345	42.548084
3503.700103	347654.018858	42.553088
3503.385953	347666.616454	42.558093
3503.617257	347668.666994	42.563098
3503.938484	347656.068346	42.568103
3503.797953	347668.333068	42.573108
3503.810602	347666.498549	42.578112
3504.173831	347633.735172	42.583117
3503.638108	347622.926386	42.588122
3503.881431	347626.298538	42.593127
3504.281167	347625.166385	42.598132
3503.631643	347622.342109	42.603136
3503.634474	347608.292111	42.608141
3504.015588	347605.763034	42.613146
3503.883527	347602.042480	42.618151
3503.961814	347608.494982	42.623156
3503.532065	347588.328496	42.628160
3503.868147	347583.464939	42.633165
3504.163487	347586.777965	42.638170
3503.930940	347569.609102	42.643175
3503.824164	347571.051338	42.648180
3503.755988	347561.263066	42.653184
3504.073813	347552.559114	42.658189
3503.883926	347554.548985	42.663194
3503.842874	347553.435613	42.668199
3504.012758	347528.211133	42.673204
3503.758561	347514.863504	42.678208
3503.930169	347513.487441	42.683213
3503.648705	347536.413486	42.688218
3503.476104	347530.484997	42.693223
3503.989933	347514.623441	42.698228
3503.529371	347518.463211	42.703232
3503.768896	347486.635585	42.708237
3503.627227	347505.034503	42.713242
3503.530457	347505.177096	42.718247
3503.628902	347504.398000	42.723252
3503.687444	347500.443688	42.728256
3503.787295	347493.123155	42.733261
3503.774367	347492.870710	42.738266
3503.873575	347484.633998	42.743271
3504.073571	347481.828123	42.748276
3503.965825	347484.110437	42.753280
3503.844097	347467.254902	42.758285
3503.647001	347454.967224	42.763290
3503.733760	347458.033259	42.768295
3503.666517	347465.730492	42.773300
3503.563765	347462.336173	42.778304
3503.843679	347451.220240	42.783309
3503.672129	347460.079314	42.788314
3503.805127	347440.969157	42.793319
3504.052784	347435.254191	42.798324
3503.761602	347440.772487	42.803329
3503.714803	347438.285601	42.808333
3503.742306	347434.107122	42.813338
3503.885563	347423.394571	42.818343
3503.786149	347405.491948	42.823348
3503.751458	347416.161953	42.828353
3503.918061	347399.057196	42.833357
3503.816575	347405.716309	42.838362
3503.926205	347401.219416	42.843367
3503.987261	347376.444761	42.848372
3503.716747	347378.371028	42.853377
3504.096590	347363.905035	42.858381
3503.531315	347382.752746	42.863386
3503.659487	347374.104203	42.868391
3503.685098	347353.891095	42.873396
3503.486584	347357.613091	42.878401
3503.511823	347356.234712	42.883405
3504.052829	347374.169413	42.888410
3503.480486	347372.223750	42.893415
3503.966708	347367.947292	42.898420
3503.731974	347359.763357	42.903425
3503.966062	347345.625829	42.908429
3503.609233	347352.325317	42.913434
3503.763464	347331.913701	42.918439
3503.773141	347337.104468	42.923444
3503.469832	347342.726499	42.928449
3503.656818	347337.581065	42.933453
3503.721710	347316.445453	42.938458
3503.479872	347298.234433	42.943463
3503.736356	347316.315943	42.948468
3503.862801	347304.613389	42.953473
3503.801158	347310.757168	42.958477
3503.622689	347304.269632	42.963482
3503.651669	347328.724723	42.968487
3504.192123	347285.752217	42.973492
3503.975440	347289.909778	42.978497
3504.128503	347293.321672	42.983501
3503.963233	347295.816706	42.988506
3504.052781	347266.303373	42.993511
3503.906611	347263.170430	42.998516
3504.022586	347270.482391	43.003521
3503.823549	347257.355051	43.008525
3503.585164	347237.692685	43.013530
3503.585274	347230.286077	43.018535
3504.035912	347226.371567	43.023540
3503.908196	347232.449443	43.028545
3503.723502	347231.613297	43.033549
3503.992497	347218.768287	43.038554
3503.831557	347207.772908	43.043559
3503.829852	347198.075873	43.048564
3503.710940	347200.894463	43.053569
3504.014954	347203.035333	43.058573
3503.885872	347191.653129	43.063578
3503.773671	347172.963432	43.068583
3504.080181	347180.143473	43.073588
3503.875999	347175.441651	43.078593
3503.607837	347176.324007	43.083597
3503.877449	347153.094329	43.088602
3503.534988	347137.393496	43.093607
3503.731079	347154.364701	43.098612
3503.663214	347150.404897	43.103617
3503.857770	347155.210119	43.108621
3503.438334	347161.003242	43.113626
3503.477514	347141.653293	43.118631
3503.649529	347144.069558	43.123636
3503.215261	347154.064665	43.128641
3503.418614	347123.489720	43.133645
3503.598064	347118.421814	43.138650
3503.459687	347119.232748	43.143655
3503.326439	347126.762295	43.148660
3503.497502	347140.072321	43.153665
3503.544853	347130.392972	43.158669
3503.533148	347144.037320	43.163674
3503.724914	347135.429592	43.168679
3503.891649	347133.876123	43.173684
3503.454739	347156.063327	43.178689
3503.587182	347135.273300	43.183693
3503.632213	347119.027607	43.188698
3503.498982	347116.452562	43.193703
3503.510145	347128.209823	43.198708
3503.601158	347121.679663	43.203713
3503.734371	347110.434142	43.208717
3504.067484	347129.598048	43.213722
3503.777440	347118.903038	43.218727
3503.918601	347118.295350	43.223732
3503.664745	347098.762643	43.228737
3503.813315	347091.968856	43.233741
3503.794057	347098.156862	43.238746
3504.054516	347078.084695	43.243751
3503.858510	347087.456740	43.248756
3503.485381	347081.050858	43.253761
3503.560560	347051.259710	43.258765
3503.682655	347068.828044	43.263770
3503.403169	347069.228597	43.268775
3503.506675	347070.230362	43.273780
3503.526013	347070.863648	43.278785
3503.821071	347081.532488	43.283789
3504.019256	347073.280069	43.288794
3503.619233	347053.439574	43.293799
3503.823941	347049.793004	43.298804
3503.918761	347056.395669	43.303809
3503.972883	347046.537069	43.308813
3503.536447	347047.216958	43.313818
3503.561814	347031.152515	43.318823
3503.781094	347014.879244	43.323828
3503.475509	347015.131209	43.328833
3503.671404	347010.976981	43.333837
3503.393876	347022.270857	43.338842
3503.707699	347030.340594	43.343847
3503.775516	347035.013149	43.348852
3503.445798	347029.618494	43.353857
3503.651825	347020.194017	43.358861
3503.435903	347022.569808	43.363866
3503.609888	347016.331947	43.368871
3503.861668	347003.107824	43.373876
3503.555327	347001.985478	43.378881
3503.620370	346990.699805	43.383885
3503.650042	346998.356327	43.388890
3503.945268	347006.250841	43.393895
3503.746295	347001.217300	43.398900
3503.552153	346987.605528	43.403905
3503.580167	346976.351159	43.408909
3503.826614	346969.949123	43.413914
3503.370692	346984.401858	43.418919
3503.527916	346987.176802	43.423924
3503.548943	346991.551328	43.428929
3503.615714	346990.879043	43.433933
3503.338388	347001.867461	43.438938
3503.893046	346989.664453	43.443943
3503.819470	346973.564731	43.448948
3503.375313	346974.602176	43.453953
3503.778550	346966.902730	43.458957
3503.368330	346970.072814	43.463962
3503.522085	346971.804758	43.468967
3503.469775	346967.587957	43.473972
3503.590621	346967.517980	43.478977
3503.774138	346968.888885	43.483981
3503.933434	346967.896542	43.488986
3503.532941	346951.288544	43.493991
3503.817021	346948.978399	43.498996
3503.565297	346952.047069	43.504001
3503.635101	346945.520242	43.509005
3503.743132	346951.637235	43.514010
3503.466955	346949.542925	43.519015
3503.478252	346951.017414	43.524020
3503.676249	346953.760461	43.529025
3503.539384	346952.280438	43.534029
3503.330220	346938.747387	43.539034
3503.450406	346930.227302	43.544039
3503.796416	346922.918683	43.549044
3503.771798	346932.187301	43.554049
3503.669635	346927.902022	43.559053
3503.763677	346923.712986	43.564058
3503.588909	346928.627520	43.569063
3503.658125	346928.031204	43.574068
3503.440968	346920.938882	43.579073
3503.675521	346901.685227	43.584077
3503.281200	346895.257222	43.589082
3503.127361	346899.964831	43.594087
3503.495265	346894.765302	43.599092
3503.388054	346906.948563	43.604097
3503.680229	346908.124123	43.609101
3503.360447	346917.286693	43.614106
3503.535536	346912.524888	43.619111
3503.607823	346920.505565	43.624116
3503.542491	346913.338334	43.629121
3503.463198	346932.363887	43.634125
3503.461544	346925.110233	43.639130
3503.748060	346916.589302	43.644135
3503.786842	346917.372230	43.649140
3503.372077	346908.529476	43.654145
3503.872208	346885.695936	43.659149
3503.773431	346887.620521	43.664154
3503.572843	346903.305533	43.669159
3503.472797	346898.332701	43.674164
3503.856636	346908.682108	43.679169
3503.929013	346882.505564	43.684173
3503.710235	346889.208732	43.689178
3503.378533	346876.738590	43.694183
3503.745674	346873.957165	43.699188
3503.639398	346870.232487	43.704193
3503.654114	346870.306551	43.709197
3503.741419	346876.325019	43.714202
3504.002649	346883.435898	43.719207
3504.078197	346858.124225	43.724212
3503.842422	346851.518435	43.729217
3504.072456	346839.112191	43.734221
3503.905228	346843.312871	43.739226
3503.514556	346820.645590	43.744231
3503.652667	346810.799123	43.749236
3503.541842	346810.816677	43.754241
3503.679277	346807.664325	43.759245
3503.482251	346825.512258	43.764250
3503.677697	346823.928790	43.769255
3503.850997	346815.578458	43.774260
3503.427919	346818.699679	43.779265
3503.713199	346790.631400	43.784269
3503.660369	346802.322488	43.789274
3503.593497	346773.546300	43.794279
3503.599822	346780.035726	43.799284
3503.702116	346806.184770	43.804289
3503.723606	346787.804693	43.809293
3503.946584	346791.129207	43.814298
3504.112752	346784.765294	43.819303
3504.040093	346773.577706	43.824308
3503.907285	346769.729952	43.829313
3503.937309	346766.772747	43.834317
3503.636485	346748.469066	43.839322
3503.216336	346741.485172	43.844327
3503.564777	346728.602039	43.849332
3503.389661	346730.895034	43.854337
3503.695060	346739.755173	43.859341
3503.703547	346741.077397	43.864346
3503.458422	346734.778502	43.869351
3503.795868	346729.736489	43.874356
3503.571008	346740.614853	43.879361
3503.970410	346741.875274	43.884365
3503.936333	346714.442856	43.889370
3503.822735	346708.581310	43.894375
3503.974116	346709.499155	43.899380
3503.569921	346722.442078	43.904385
3503.779879	346702.021427	43.909389
3503.464972	346688.046888	43.914394
3503.599075	346688.051173	43.919399
3503.746645	346676.472413	43.924404
3503.689316	346679.230387	43.929409
3503.763817	346679.447715	43.934413
3503.733179	346683.346834	43.939418
3503.497817	346687.456487	43.944423
3503.808692	346675.419216	43.949428
3503.618486	346655.214528	43.954433
3503.815258	346646.580482	43.959437
3503.789872	346656.383770	43.964442
3503.991246	346661.569745	43.969447
3504.130280	346645.283602	43.974452
3503.542744	346626.668875	43.979457
3503.848886	346626.213267	43.984461
3503.936039	346619.861828	43.989466
3503.659703	346616.749428	43.994471
3503.694617	346634.102606	43.999476
3503.941483	346622.024538	44.004481
3503.865060	346603.939860	44.009485
3503.630853	346609.449229	44.014490
3503.933362	346605.049043	44.019495
3504.086104	346601.385207	44.024500
3503.677437	346590.861568	44.029505
3503.670871	346568.998850	44.034509
3504.028821	346570.062208	44.039514
3503.971886	346570.962084	44.044519
3504.161123	346562.405575	44.049524
3503.853499	346541.175852	44.054529
3503.752902	346538.926506	44.059533
3503.757928	346535.413283	44.064538
3503.662506	346527.843519	44.069543
3503.687678	346531.606562	44.074548
3503.599611	346516.043508	44.079553
3503.410947	346506.732250	44.084557
3503.749199	346505.507986	44.089562
3503.460821	346509.931465	44.094567
3503.722082	346501.872612	44.099572
3503.484834	346504.429965	44.104577
3503.619526	346501.023503	44.109581
3503.268806	346509.809239	44.114586
3503.636719	346510.896476	44.119591
3503.670098	346508.524137	44.124596
3503.792646	346507.766670	44.129601
3504.017738	346482.685715	44.134605
3503.989486	346482.970194	44.139610
3503.702229	346483.804674	44.144615
3503.786353	346482.671491	44.149620
3503.772109	346474.961623	44.154625
3503.913915	346449.435673	44.159629
3503.998796	346457.236255	44.164634
3503.759615	346455.161531	44.169639
3504.072528	346441.927614	44.174644
3503.338293	346430.742741	44.179649
3503.483413	346414.684645	44.184653
3503.532971	346428.752174	44.189658
3503.407558	346426.303125	44.194663
3503.768660	346420.697386	44.199668
3503.627516	346425.072142	44.204673
3503.453261	346425.430609	44.209677
3503.435964	346429.276731	44.214682
3503.558696	346428.239254	44.219687
3503.722947	346409.658318	44.224692
3503.713417	346416.226649	44.229697
3503.620956	346395.980964	44.234701
3503.655105	346393.073992	44.239706
3503.528284	346392.126873	44.244711
3503.979533	346388.543095	44.249716
3503.706106	346406.225069	44.254721
3503.902680	346384.661050	44.259725
3503.638812	346372.740033	44.264730
3503.528651	346380.571460	44.269735
3503.819204	346370.344479	44.274740
3503.703237	346373.111738	44.279745
3504.029328	346361.962841	44.284749
3503.849809	346360.845883	44.289754
3503.785933	346336.981374	44.294759
3504.049594	346333.478155	44.299764
3503.680243	346339.619780	44.304769
3504.028261	346333.048898	44.309773
3503.631497	346329.064676	44.314778
3503.821135	346302.258463	44.319783
3503.932117	346294.452415	44.324788
3503.709374	346294.564021	44.329793
3503.929088	346298.423587	44.334797
3503.844261	346298.742464	44.339802
3503.838741	346274.665081	44.344807
3503.557873	346277.789300	44.349812
3503.404059	346278.679044	44.354817
3503.889215	346259.003764	44.359821
3503.837826	346261.582649	44.364826
3503.553728	346267.710803	44.369831
3503.635189	346264.312743	44.374836
3503.579740	346254.140443	44.379841
3503.660982	346240.994012	44.384845
3503.746735	346239.911472	44.389850
3503.441269	346237.465428	44.394855
3503.454809	346234.281726	44.399860
3503.247643	346248.593508	44.404865
3503.477513	346245.884661	44.409869
3503.487658	346237.763661	44.414874
3503.181769	346249.189436	44.419879
3503.425017	346245.740344	44.424884
3503.148394	346261.335741	44.429889
3503.440572	346254.315529	44.434893
3503.311412	346257.543029	44.439898
3503.215361	346254.707540	44.444903
3503.333212	346254.765300	44.449908
3503.074723	346267.456215	44.454913
3503.455651	346254.491482	44.459917
3503.734296	346264.195866	44.464922
3503.367533	346261.377722	44.469927
3503.802551	346262.225280	44.474932
3503.659747	346268.483813	44.479937
3503.744411	346243.221333	44.484941
3503.542604	346244.373193	44.489946
3503.592236	346234.387899	44.494951
3503.582467	346236.909300	44.499956
3503.495014	346231.756249	44.504961
3503.657261	346224.400236	44.509965
3503.354976	346244.224854	44.514970
3503.791943	346244.639407	44.519975
3503.861658	346233.836449	44.524980
3503.489870	346220.990710	44.529985
3503.271319	346210.971452	44.534989
3503.521860	346204.034175	44.539994
3503.314668	346199.485466	44.544999
3503.641872	346208.698579	44.550004
3503.403003	346209.932657	44.555009
3503.615007	346197.121881	44.560013
3503.511357	346198.869090	44.565018
3503.176165	346224.451244	44.570023
3503.665546	346209.713114	44.575028
3503.588684	346215.604889	44.580033
3503.559251	346210.748097	44.585037
3503.356849	346224.142832	44.590042
3503.370099	346222.028191	44.595047
3503.721104	346221.641846	44.600052
3503.716635	346212.352326	44.605057
3503.529763	346183.314833	44.610061
3503.744017	346197.967247	44.615066
3503.915619	346189.667998	44.620071
3504.096404	346178.796565	44.625076
3503.809896	346204.956445	44.630081
3503.601744	346174.140618	44.635085
3503.668813	346171.126619	44.640090
3503.735179	346153.426470	44.645095
3503.762852	346174.191606	44.650100
3503.606310	346157.163019	44.655105
3503.310338	346160.493254	44.660109
3503.550934	346181.224726	44.665114
3503.521513	346171.939144	44.670119
3503.880202	346135.968576	44.675124
3503.841251	346136.712899	44.680129
3503.879895	346140.855629	44.685133
3503.807287	346139.670860	44.690138
3503.735478	346128.457560	44.695143
3503.978445	346122.285054	44.700148
3503.901426	346111.403461	44.705153
3503.706575	346099.496928	44.710157
3503.536038	346101.152903	44.715162
3503.277805	346110.305871	44.720167
3503.487052	346094.110284	44.725172
3503.612269	346115.140000	44.730177
3503.741485	346099.237048	44.735181
3503.614135	346090.272369	44.740186
3503.615375	346080.523775	44.745191
3503.701800	346070.863522	44.750196
3503.565448	346074.906660	44.755201
3503.433431	346077.421942	44.760205
3503.548577	346079.058205	44.765210
3503.550167	346082.010515	44.770215
3504.055130	346083.356074	44.775220
3503.690681	346072.621726	44.780225
3503.616048	346055.605612	44.785229
3503.437874	346047.412547	44.790234
3503.455590	346051.762215	44.795239
3503.659201	346045.366848	44.800244
3503.278141	346059.171659	44.805249
3503.690071	346054.677774	44.810253
3503.463169	346052.270207	44.815258
3503.620923	346058.023095	44.820263
3503.527720	346059.692298	44.825268
3503.182306	346056.030826	44.830273
3503.161737	346054.125148	44.835277
3503.439658	346062.404321	44.840282
3503.327472	346059.444109	44.845287
3503.690146	346055.237993	44.850292
3503.539328	346068.599156	44.855297
3503.783809	346034.301014	44.860301
3503.745937	346030.260032	44.865306
3503.896578	346029.778099	44.870311
3503.684378	346017.696122	44.875316
3503.627079	346028.599035	44.880321
3503.629639	346028.191419	44.885325
3503.799779	346012.027444	44.890330
3503.216514	346004.585643	44.895335
3503.513657	345996.342878	44.900340
3503.368958	345997.282090	44.905345
3503.365170	345995.781004	44.910349
3503.714911	346000.459977	44.915354
3503.381729	346008.504884	44.920359
3503.575414	346003.918234	44.925364
3503.502328	345999.679194	44.930369
3503.515928	346012.785301	44.935373
3503.747882	346019.519123	44.940378
3503.323050	346016.481072	44.945383
3503.967960	345999.834789	44.950388
3503.508182	345993.671560	44.955393
3503.568932	345972.510654	44.960397
3503.613762	345969.169273	44.965402
3503.617659	345988.156533	44.970407
3503.640415	345972.270377	44.975412
3503.468585	345985.965768	44.980417
3503.611819	345973.394891	44.985421
3503.617396	345982.277096	44.990426
3503.569723	345973.554331	44.995431
3503.906831	345961.461858	45.000436
3503.523854	345955.490105	45.005441
3503.625166	345950.994414	45.010445
3503.469832	345952.927972	45.015450
3503.450367	345944.938876	45.020455
3503.701363	345959.992789	45.025460
3503.705342	345958.694096	45.030465
3503.699840	345947.190296	45.035469
3503.569975	345959.046451	45.040474
3503.472646	345948.066226	45.045479
3503.557596	345924.890699	45.050484
3503.797854	345928.492513	45.055489
3503.643637	345929.993195	45.060493
3503.568660	345922.318307	45.065498
3503.262137	345934.075132	45.070503
3503.386369	345940.215125	45.075508
3503.566041	345941.739379	45.080513
3503.788378	345935.951909	45.085517
3503.855578	345933.370576	45.090522
3503.681666	345914.308432	45.095527
3503.836994	345894.125208	45.100532
3503.756754	345897.574070	45.105537
3504.031388	345905.166557	45.110541
3503.739938	345903.532775	45.115546
3503.548258	345882.411744	45.120551
3503.746584	345865.123345	45.125556
3503.429003	345865.911721	45.130561
3503.619068	345870.590496	45.135565
3503.701641	345867.395860	45.140570
3503.489875	345867.887525	45.145575
3503.530362	345862.306968	45.150580
3503.656813	345877.686027	45.155585
3503.361583	345861.621036	45.160589
3503.381451	345882.871116	45.165594
3503.631210	345873.337726	45.170599
3503.607253	345845.063347	45.175604
3503.398646	345850.848723	45.180609
3503.640823	345838.313080	45.185613
3503.710560	345847.006991	45.190618
3503.720634	345837.104241	45.195623
3503.417112	345834.861496	45.200628
3503.509373	345843.450035	45.205633
3503.834497	345832.504812	45.210637
3503.593074	345842.647828	45.215642
3503.545461	345840.135548	45.220647
3503.725505	345810.225366	45.225652
3503.502250	345817.412973	45.230657
3503.510863	345809.724855	45.235661
3503.456285	345813.984159	45.240666
3503.350989	345810.666504	45.245671
3503.625112	345804.539945	45.250676
3503.325598	345802.525641	45.255681
3503.630596	345801.281167	45.260685
3503.534206	345817.229984	45.265690
3503.414586	345821.754100	45.270695
3503.682685	345813.414089	45.275700
3503.299747	345811.794769	45.280705
3503.457793	345803.243078	45.285709
3503.558092	345788.311824	45.290714
3503.436448	345802.202949	45.295719
3503.656290	345788.856332	45.300724
3503.444250	345782.832084	45.305729
3503.437792	345792.937962	45.310733
3503.763247	345789.679470	45.315738
3503.490706	345794.049593	45.320743
3503.840794	345783.711285	45.325748
3503.625156	345801.409760	45.330753
3503.930169	345774.941404	45.335757
3503.736167	345775.608432	45.340762
3503.424778	345760.716805	45.345767
3503.696977	345756.244988	45.350772
3503.601665	345754.809271	45.355777
3503.411121	345750.868765	45.360781
3503.978820	345758.593109	45.365786
3503.705881	345770.497376	45.370791
3503.770927	345745.975916	45.375796
3503.474069	345747.499154	45.380801
3503.684955	345735.121154	45.385805
3503.829337	345737.821830	45.390810
3503.597207	345746.487121	45.395815
3503.654417	345742.660163	45.400820
3503.330675	345752.154432	45.405825
3504.106524	345746.915760	45.410829
3503.808807	345732.098322	45.415834
3503.276538	345707.874904	45.420839
3503.677201	345699.030311	45.425844
3503.735004	345708.795156	45.430849
3503.930016	345699.677640	45.435853
3504.017988	345700.274637	45.440858
3503.756729	345696.370760	45.445863
3503.636258	345670.682308	45.450868
3503.427884	345689.346883	45.455873
3503.484625	345657.878030	45.460877
3503.560235	345674.054224	45.465882
3503.580981	345688.304659	45.470887
3504.062488	345656.514122	45.475892
3503.604204	345681.479650	45.480897
3503.655930	345653.829538	45.485901
3503.696920	345624.806647	45.490906
3503.773468	345652.792903	45.495911
3503.802360	345637.058403	45.500916
3503.578277	345636.050289	45.505921
3503.835123	345626.490285	45.510925
3504.098195	345631.437520	45.515930
3503.701688	345623.915238	45.520935
3503.662596	345600.301037	45.525940
3503.654270	345634.027653	45.530945
3503.873019	345609.736366	45.535949
3503.700551	345621.879309	45.540954
3503.356354	345602.513095	45.545959
3503.915859	345568.470311	45.550964
3503.360905	345589.327767	45.555969
3503.634314	345583.023127	45.560973
3503.687949	345581.462045	45.565978
3503.596317	345579.491227	45.570983
3503.793103	345589.106854	45.575988
3503.710743	345591.359776	45.580993
3503.471010	345554.210804	45.585997
3503.681128	345554.966663	45.591002
3503.356500	345560.134083	45.596007
3503.652650	345545.833584	45.601012
3503.347501	345556.139443	45.606017
3503.386437	345545.977550	45.611021
3503.702087	345541.193411	45.616026
3503.146938	345569.279575	45.621031
3503.451455	345547.341836	45.626036
3503.442828	345548.132279	45.631041
3503.342292	345552.093431	45.636045
3503.229704	345562.343393	45.641050
3503.355667	345570.901191	45.646055
3503.591433	345554.217653	45.651060
3503.357043	345560.007133	45.656065
3503.684468	345563.213393	45.661069
3503.697114	345572.094543	45.666074
3503.344687	345536.846902	45.671079
3503.601965	345537.340775	45.676084
3503.784632	345528.657886	45.681089
3503.706522	345526.990366	45.686093
3503.705868	345534.600970	45.691098
3503.915797	345528.713609	45.696103
3503.661890	345519.972475	45.701108
3503.619264	345530.694990	45.706113
3503.666323	345504.445464	45.711117
3503.871913	345513.321572	45.716122
3503.473821	345483.629888	45.721127
3503.662173	345500.984601	45.726132
3503.230022	345518.488314	45.731137
3503.767776	345498.499024	45.736141
3503.764585	345504.913738	45.741146
3503.709185	345512.940250	45.746151
3503.870849	345469.924463	45.751156
3503.265337	345481.703195	45.756161
3503.590320	345461.518452	45.761165
3503.240979	345465.697116	45.766170
3503.281365	345455.229541	45.771175
3503.566180	345477.634178	45.776180
3503.522776	345477.564714	45.781185
3503.594831	345470.146506	45.786189
3503.317574	345483.553246	45.791194
3503.405970	345487.917235	45.796199
3503.623761	345475.156292	45.801204
3503.268424	345508.581498	45.806209
3503.371906	345469.927385	45.811213
3503.404279	345491.761053	45.816218
3503.604070	345479.181127	45.821223
3503.563991	345499.906310	45.826228
3503.137973	345457.085235	45.831233
3503.446937	345480.071475	45.836237
3503.650168	345450.310160	45.841242
3503.142644	345450.339525	45.846247
3503.748599	345437.899003	45.851252
3503.357002	345460.741475	45.856257
3503.457683	345448.380836	45.861261
3503.613524	345446.319983	45.866266
3503.365694	345469.954222	45.871271
3503.649804	345452.473966	45.876276
3503.086101	345450.679589	45.881281
3503.510897	345460.081017	45.886285
3503.637551	345446.799961	45.891290
3503.798548	345465.278946	45.896295
3504.091892	345437.590533	45.901300
3503.522200	345427.855731	45.906305
3503.064383	345435.105921	45.911309
3503.481847	345426.004100	45.916314
3503.387947	345414.870514	45.921319
3503.861088	345418.435541	45.926324
3503.574778	345427.287617	45.931329
3503.350213	345418.821813	45.936333
3503.737229	345428.763735	45.941338
3503.166891	345408.669615	45.946343
3503.260820	345431.740775	45.951348
3503.239688	345429.427916	45.956353
3503.440487	345415.320631	45.961357
3503.561167	345438.183935	45.966362
3503.483082	345427.658725	45.971367
3503.749396	345427.693015	45.976372
3503.653812	345437.380342	45.981377
3503.559162	345400.921022	45.986381
3503.389273	345400.337039	45.991386
3503.210718	345409.732051	45.996391
3503.399861	345397.535588	46.001396
3503.239782	345417.999787	46.006401
3503.520961	345411.261197	46.011405
3503.633471	345393.578974	46.016410
3503.787440	345408.215666	46.021415
3503.562858	345409.854752	46.026420
3503.557273	345411.077418	46.031425
3503.713630	345406.343904	46.036429
3503.716262	345407.717990	46.041434
3503.351462	345397.518088	46.046439
3503.668522	345377.996350	46.051444
3503.376188	345369.515799	46.056449
3503.707053	345368.139961	46.061453
3503.509680	345388.406441	46.066458
3503.613793	345377.776058	46.071463
3503.801815	345364.128937	46.076468
3503.418344	345370.247443	46.081473
3503.714315	345373.229608	46.086477
3503.765119	345379.737612	46.091482
3503.405490	345364.853510	46.096487
3503.737719	345343.140392	46.101492
3503.657148	345343.942211	46.106497
3503.459291	345344.151697	46.111501
3503.442888	345343.492541	46.116506
3503.514767	345342.641257	46.121511
3503.559401	345346.528566	46.126516
3503.362392	345349.232326	46.131521
3503.177805	345342.567364	46.136525
3503.713959	345340.751819	46.141530
3503.520975	345348.698293	46.146535
3503.642497	345349.493615	46.151540
3503.602033	345347.489246	46.156545
3503.646090	345325.159899	46.161549
3503.366286	345326.044122	46.166554
3503.609029	345310.759336	46.171559
3503.804390	345311.822969	46.176564
3503.614388	345313.991107	46.181569
3503.716407	345321.025538	46.186573
3503.487146	345323.454413	46.191578
3503.155806	345324.932207	46.196583
3504.008168	345322.837592	46.201588
3503.430886	345316.412882	46.206593
3503.586546	345301.396392	46.211597
3503.739845	345296.256102	46.216602
3503.378260	345305.756427	46.221607
3503.873559	345294.020604	46.226612
3503.166031	345312.942386	46.231617
3503.251834	345306.743735	46.236621
3503.847978	345306.649520	46.241626
3503.599767	345301.878146	46.246631
3503.705099	345293.181996	46.251636
3503.565018	345305.396244	46.256641
3503.313640	345284.004449	46.261645
3503.437975	345269.196528	46.266650
3503.395667	345266.836104	46.271655
3503.434772	345263.979198	46.276660
3503.146960	345276.369527	46.281665
3503.525055	345263.914085	46.286669
3503.702945	345258.057216	46.291674
3503.200854	345276.946530	46.296679
3503.455224	345269.244941	46.301684
3503.501685	345270.993899	46.306689
3503.059941	345290.433639	46.311693
3503.320931	345277.742182	46.316698
3503.468064	345281.944182	46.321703
3503.663247	345264.376116	46.326708
3503.690814	345283.410770	46.331713
3503.681331	345280.459734	46.336717
3503.874591	345274.625889	46.341722
3503.556544	345265.411246	46.346727
3503.661115	345250.937337	46.351732
3503.606029	345246.517224	46.356737
3503.327272	345237.627256	46.361741
3503.567419	345235.094910	46.366746
3503.147337	345243.764537	46.371751
3503.839250	345240.320813	46.376756
3503.335306	345252.567145	46.381761
3503.611070	345247.102051	46.386765
3503.702448	345243.167846	46.391770
3503.401940	345245.811614	46.396775
3503.506824	345252.285630	46.401780
3503.538288	345252.815206	46.406785
3503.376328	345230.136595	46.411789
3503.224128	345226.062725	46.416794
3503.525470	345221.535354	46.421799
3503.452061	345215.896382	46.426804
3503.340779	345214.717708	46.431809
3503.637644	345220.754124	46.436813
3503.650592	345229.177120	46.441818
3503.464715	345221.316048	46.446823
3503.418993	345227.279359	46.451828
3503.385330	345225.681162	46.456833
3503.202150	345220.034092	46.461837
3503.261634	345234.813031	46.466842
3503.434084	345234.047658	46.471847
3503.376410	345236.067612	46.476852
3503.246604	345236.495418	46.481857
3503.320406	345228.949637	46.486861
3503.561503	345223.719101	46.491866
3503.114502	345230.331276	46.496871
3503.447731	345223.482623	46.501876
3503.326796	345223.069071	46.506881
3503.395793	345225.323531	46.511885
3503.596506	345237.178477	46.516890
3503.488329	345242.006267	46.521895
3503.706293	345235.913980	46.526900
3503.312115	345243.765010	46.531905
3503.252779	345253.344824	46.536909
3503.524473	345244.596912	46.541914
3503.230619	345247.239628	46.546919
3503.467645	345236.206409	46.551924
3503.456338	345229.717664	46.556929
3503.461081	345223.480913	46.561933
3503.514065	345219.756402	46.566938
3503.426181	345219.668517	46.571943
3503.684105	345210.362807	46.576948
3503.529570	345217.386904	46.581953
3503.538708	345225.912315	46.586957
3503.478674	345215.129682	46.591962
3503.477075	345214.722717	46.596967
3503.554023	345211.859825	46.601972
3503.673912	345225.840168	46.606977
3503.471274	345224.472311	46.611981
3503.475229	345229.511453	46.616986
3503.040368	345229.071172	46.621991
3503.455257	345224.500397	46.626996
3503.502390	345217.671520	46.632001
3503.203587	345218.991453	46.637005
3503.492798	345215.204143	46.642010
3503.533281	345210.259854	46.647015
3503.505829	345184.760107	46.652020
3503.413354	345187.218269	46.657025
3503.696177	345193.740519	46.662029
3503.483126	345192.399762	46.667034
3503.539756	345198.270535	46.672039
3503.707295	345182.895791	46.677044
3503.706928	345200.153163	46.682049
3503.454443	345215.719571	46.687053
3503.795278	345185.376397	46.692058
3503.485851	345178.222088	46.697063
3503.372086	345167.575206	46.702068
3503.706316	345178.110941	46.707073
3503.678698	345162.945218	46.712077
3503.492518	345165.621821	46.717082
3503.626559	345177.690946	46.722087
3503.709035	345161.413328	46.727092
3503.807104	345156.790823	46.732097
3503.570210	345156.293790	46.737101
3503.375251	345148.332330	46.742106
3503.530919	345132.043134	46.747111
3503.787541	345120.930435	46.752116
3503.631993	345127.598357	46.757121
3503.777781	345118.717612	46.762125
3504.016065	345126.570480	46.767130
3503.204352	345138.280067	46.772135
3503.622892	345125.029152	46.777140
3503.456006	345120.524891	46.782145
3503.390598	345109.692181	46.787149
3503.708349	345114.325377	46.792154
3503.482944	345112.172067	46.797159
3503.587011	345095.941925	46.802164
3503.523365	345100.711779	46.807169
3503.522556	345101.628258	46.812173
3503.620205	345105.201762	46.817178
3503.441243	345108.284479	46.822183
3503.992066	345106.924767	46.827188
3503.462576	345098.023512	46.832193
3503.485379	345097.816314	46.837197
3503.406617	345086.425739	46.842202
3503.387997	345074.007523	46.847207
3503.643245	345071.905488	46.852212
3503.305310	345074.555181	46.857217
3503.286086	345080.692491	46.862221
3503.584013	345074.409373	46.867226
3503.454971	345087.538239	46.872231
3503.641543	345076.716592	46.877236
3503.779410	345076.058497	46.882241
3503.685880	345074.444308	46.887245
3503.849908	345071.949443	46.892250
3503.613017	345058.216708	46.897255
3503.730779	345051.478459	46.902260
3503.334429	345048.130414	46.907265
3503.236569	345047.407774	46.912269
3503.702156	345043.516208	46.917274
3503.772182	345046.101405	46.922279
3503.915808	345044.907881	46.927284
3503.708041	345044.380789	46.932289
3503.848923	345032.853666	46.937293
3503.853115	345016.741104	46.942298
3503.502826	345023.617999	46.947303
3503.779085	344998.502862	46.952308
3503.388592	345007.702365	46.957313
3503.543350	345021.142724	46.962317
3504.068074	345012.074788	46.967322
3503.541289	345004.114863	46.972327
3503.780280	344985.063496	46.977332
3503.755514	344971.246298	46.982337
3503.441842	344977.455623	46.987341
3503.531640	344978.434138	46.992346
3503.680037	344970.011118	46.997351
3503.276446	344970.074958	47.002356
3503.084571	344978.861265	47.007361
3502.956168	344975.903561	47.012365
3503.493140	344981.036630	47.017370
3503.072764	344981.332203	47.022375
3503.158857	344976.584310	47.027380
3503.054926	344975.608095	47.032385
3503.460991	344990.077770	47.037389
3503.355190	344982.483991	47.042394
3503.241031	344978.734983	47.047399
3503.339378	344985.031889	47.052404
3503.184632	344981.034765	47.057409
3503.345012	345012.418816	47.062413
3503.509252	344982.510709	47.067418
3503.597220	344996.343432	47.072423
3503.335333	345004.733551	47.077428
3503.485586	344989.717836	47.082433
3503.523877	344996.915101	47.087437
3503.037156	345005.748018	47.092442
3503.334733	344986.763749	47.097447
3503.646287	344990.074363	47.102452
3503.675241	345008.268929	47.107457
3503.594404	344996.242332	47.112461
3503.268852	344992.730371	47.117466
3503.555290	344980.543893	47.122471
3503.490764	345020.668528	47.127476
3503.526190	344967.312839	47.132481
3503.406495	344980.771144	47.137485
3503.392074	344949.389520	47.142490
3502.824170	344982.314113	47.147495
3503.305562	344970.224078	47.152500
3503.197168	344993.021958	47.157505
3503.357810	344996.916403	47.162509
3503.436863	344997.794804	47.167514
3503.367940	344992.918700	47.172519
3503.361291	344976.222416	47.177524
3503.120883	344989.241644	47.182529
3503.264202	345004.261920	47.187533
3503.753574	345013.475039	47.192538
3503.278465	344986.442420	47.197543
3503.342929	344974.774647	47.202548
3503.265236	344980.666678	47.207553
3503.209579	344984.671680	47.212557
3503.372330	344986.631341	47.217562
3503.183932	344972.509120	47.222567
3503.560432	344972.551443	47.227572
3503.505292	344976.403644	47.232577
3503.423247	344981.329137	47.237581
3503.562843	344970.489444	47.242586
3503.303956	344975.595616	47.247591
3503.847902	344982.763846	47.252596
3503.902924	344987.922202	47.257601
3503.508923	344991.726161	47.262605
3503.935075	344992.142435	47.267610
3503.815361	344975.387665	47.272615
3503.816655	344957.366547	47.277620
3503.608250	344950.247146	47.282625
3503.526709	344956.928841	47.287629
3503.705069	344950.359173	47.292634
3503.511867	344951.076990	47.297639
3503.718258	344949.288115	47.302644
3503.406396	344948.344773	47.307649
3503.296042	344940.089923	47.312653
3503.536806	344922.132748	47.317658
3503.342381	344921.552639	47.322663
3503.485775	344912.519522	47.327668
3503.484877	344911.679737	47.332673
3503.760445	344918.483152	47.337677
3503.774170	344917.539242	47.342682
3503.520210	344927.149879	47.347687
3503.714428	344927.424647	47.352692
3503.676232	344916.943946	47.357697
3503.520847	344911.394264	47.362701
3503.675062	344903.606648	47.367706
3503.730206	344907.950485	47.372711
3503.811513	344889.662163	47.377716
3503.604180	344899.189073	47.382721
3503.703052	344899.020755	47.387725
3503.554006	344893.317350	47.392730
3503.434773	344899.775930	47.397735
3503.682734	344895.486053	47.402740
3503.679374	344881.996343	47.407745
3503.488010	344868.587260	47.412749
3503.821748	344862.858432	47.417754
3503.679864	344855.753955	47.422759
3503.710303	344852.796586	47.427764
3503.396606	344867.863697	47.432769
3503.387219	344862.876356	47.437773
3503.797551	344868.360350	47.442778
3503.514901	344877.339197	47.447783
3503.588669	344857.244869	47.452788
3503.395856	344836.581798	47.457793
3503.431932	344831.383641	47.462797
3503.622970	344834.586050	47.467802
3503.528659	344837.935385	47.472807
3503.946980	344830.055098	47.477812
3503.580585	344829.833070	47.482817
3503.622321	344839.371520	47.487821
3503.745060	344832.021578	47.492826
3503.721680	344824.923816	47.497831
3503.650203	344808.797708	47.502836
3503.378742	344803.342727	47.507841
3503.404632	344799.087952	47.512845
3503.578801	344810.209032	47.517850
3503.100829	344803.895832	47.522855
3503.644589	344796.224790	47.527860
3503.389965	344805.581018	47.532865
3503.446848	344806.030219	47.537869
3503.762291	344794.628172	47.542874
3503.434215	344805.650482	47.547879
3503.421610	344799.238256	47.552884
3503.480744	344798.796233	47.557889
3503.809973	344787.926526	47.562893
3503.604794	344770.879769	47.567898
3503.345335	344776.851463	47.572903
3503.670978	344770.156677	47.577908
3503.547523	344773.561530	47.582913
3503.592740	344782.234023	47.587917
3503.595694	344777.448351	47.592922
3503.338836	344785.150465	47.597927
3503.533767	344775.523750	47.602932
3503.775763	344777.750878	47.607937
3503.393095	344775.724231	47.612941
3503.476665	344782.990723	47.617946
3503.441293	344783.352696	47.622951
3503.726641	344757.065163	47.627956
3503.414762	344748.587612	47.632961
3503.316532	344750.944888	47.637965
3503.659917	344729.967929	47.642970
3503.499816	344733.454939	47.647975
3503.930466	344732.725099	47.652980
3503.625233	344743.158381	47.657985
3503.546696	344745.919800	47.662989
3503.695063	344736.911322	47.667994
3503.347644	344747.631261	47.672999
3503.583338	344744.285089	47.678004
3503.308645	344704.035787	47.683009
3503.333570	344722.663786	47.688013
3503.106229	344703.915135	47.693018
3502.972148	344724.680906	47.698023
3503.279236	344734.126515	47.703028
3503.136993	344746.468488	47.708033
3503.254494	344748.944379	47.713037
3503.842852	344741.113558	47.718042
3503.310684	344742.572210	47.723047
3503.998611	344753.357544	47.728052
3503.474072	344704.824478	47.733057
3503.435467	344723.946136	47.738061
3503.549856	344721.688184	47.743066
3503.494148	344723.249683	47.748071
3503.484202	344712.179050	47.753076
3503.283527	344713.508934	47.758081
3503.245170	344730.365196	47.763085
3503.546947	344707.536708	47.768090
3503.435095	344724.862752	47.773095
3503.705756	344723.980032	47.778100
3503.865322	344714.384352	47.783105
3503.496452	344698.381590	47.788109
3503.607850	344695.615041	47.793114
3503.400827	344678.212201	47.798119
3503.595171	344697.195225	47.803124
3503.871665	344674.243454	47.808129
3503.268378	344702.184922	47.813133
3503.675886	344684.226767	47.818138
3503.361147	344690.792639	47.823143
3503.796276	344702.177924	47.828148
3503.310129	344686.830036	47.833153
3503.302302	344712.870165	47.838157
3503.502117	344678.832825	47.843162
3503.479735	344704.875259	47.848167
3503.463248	344689.224039	47.853172
3503.396740	344676.278787	47.858177
3503.325717	344672.064778	47.863181
3503.625634	344664.025014	47.868186
3503.513719	344665.697215	47.873191
3503.614531	344658.808880	47.878196
3503.511419	344662.261430	47.883201
3503.375694	344662.206561	47.888205
3503.544771	344655.841956	47.893210
3503.144764	344662.446765	47.898215
3503.446005	344665.631761	47.903220
3503.586223	344668.969481	47.908225
3503.179625	344660.990507	47.913229
3503.531761	344660.145813	47.918234
3503.086959	344669.099420	47.923239
3503.462058	344656.771591	47.928244
3503.398441	344662.126905	47.933249
3503.711205	344673.684262	47.938253
3503.335121	344682.474283	47.943258
3503.631295	344666.875440	47.948263
3503.704690	344660.576869	47.953268
3503.707135	344644.591749	47.958273
3503.759413	344641.936359	47.963277
3503.973263	344618.765388	47.968282
3503.355226	344623.062953	47.973287
3503.756233	344630.075651	47.978292
3503.506654	344633.678626	47.983297
3503.419946	344624.249134	47.988301
3503.557022	344632.347150	47.993306
3502.890171	344628.074615	47.998311
3503.558327	344619.671187	48.003316
3503.343063	344626.094071	48.008321
3503.215363	344647.902453	48.013325
3503.711878	344640.620662	48.018330
3503.331159	344620.521746	48.023335
3503.146858	344626.023411	48.028340
3503.539415	344599.846125	48.033345
3503.430771	344592.150932	48.038349
3503.338805	344608.328460	48.043354
3502.991188	344598.558410	48.048359
3503.284137	344623.125633	48.053364
3503.619524	344609.225958	48.058369
3503.316525	344593.594555	48.063373
3503.496668	344614.565223	48.068378
3503.407324	344588.336851	48.073383
3503.255505	344622.748525	48.078388
3503.405148	344606.765577	48.083393
3503.307855	344603.293867	48.088397
3503.372707	344626.319035	48.093402
3503.200905	344597.761985	48.098407
3503.228511	344628.709070	48.103412
3503.329208	344608.763121	48.108417
3503.255910	344621.857824	48.113421
3503.781716	344609.887961	48.118426
3503.567759	344630.080964	48.123431
3503.745777	344589.378211	48.128436
3503.517783	344622.020184	48.133441
3503.271351	344627.786207	48.138445
3503.511275	344623.701209	48.143450
3503.216951	344616.977152	48.148455
3503.625930	344628.290226	48.153460
3503.379972	344635.227031	48.158465
3503.404770	344630.106999	48.163469
3503.643992	344611.335463	48.168474
3503.193625	344644.470743	48.173479
3503.430506	344612.234699	48.178484
3503.426199	344626.642075	48.183489
3503.409849	344582.432014	48.188493
3503.716283	344600.430116	48.193498
3503.341587	344569.945213	48.198503
3503.467462	344606.985609	48.203508
3503.186457	344580.711175	48.208513
3503.468828	344577.204893	48.213517
3503.584125	344591.211566	48.218522
3503.583589	344598.644099	48.223527
3503.514947	344581.372073	48.228532
3503.463014	344611.237242	48.233537
3503.487218	344592.525147	48.238541
3503.858879	344594.859049	48.243546
3503.694384	344603.742897	48.248551
3503.919270	344589.682513	48.253556
3503.732893	344576.908912	48.258561
3503.346348	344572.566603	48.263565
3503.419037	344564.817285	48.268570
3503.389760	344561.614808	48.273575
3503.423254	344577.339800	48.278580
3503.435138	344572.883595	48.283585
3503.562523	344564.794734	48.288589
3504.016768	344552.887080	48.293594
3503.672146	344560.628552	48.298599
3503.842482	344539.755244	48.303604
3503.647796	344528.230167	48.308609
3503.392920	344527.888693	48.313613
3503.523481	344525.068199	48.318618
3503.526969	344527.663939	48.323623
3503.486271	344528.535826	48.328628
3503.283382	344532.589588	48.333633
3503.420601	344529.131705	48.338637
3503.561512	344525.749599	48.343642
3503.218757	344558.384297	48.348647
3503.818947	344526.956188	48.353652
3503.331344	344533.345778	48.358657
3503.422218	344550.334381	48.363661
3503.845453	344533.748183	48.368666
3503.890186	344512.283839	48.373671
3503.617007	344499.982107	48.378676
3503.517038	344506.234056	48.383681
3503.740240	344507.955094	48.388685
3503.655695	344505.957666	48.393690
3503.220508	344504.753826	48.398695
3503.293877	344494.713574	48.403700
3503.150155	344509.295740	48.408705
3503.316992	344504.433230	48.413709
3503.173349	344504.405066	48.418714
3503.360703	344511.298835	48.423719
3503.410431	344496.757050	48.428724
3503.435557	344512.559743	48.433729
3503.461329	344508.483140	48.438733
3503.457919	344500.109507	48.443738
3503.372876	344515.878709	48.448743
3503.814942	344496.591451	48.453748
3503.664988	344482.183046	48.458753
3503.263543	344461.985538	48.463757
3503.474635	344473.864450	48.468762
3503.482727	344479.564794	48.473767
3503.754941	344470.027626	48.478772
3503.302775	344475.648014	48.483777
3503.166719	344477.985829	48.488781
3503.396582	344475.913240	48.493786
3503.407593	344475.300648	48.498791
3503.473318	344474.323056	48.503796
3503.471988	344476.028686	48.508801
3502.935088	344486.549546	48.513805
3503.321382	344474.270816	48.518810
3503.541559	344480.573969	48.523815
3503.573598	344477.081804	48.528820
3503.353458	344483.963639	48.533825
3503.516468	344464.109603	48.538829
3503.651520	344474.015162	48.543834
3503.331275	344485.774446	48.548839
3503.749372	344476.341483	48.553844
3503.680206	344463.014802	48.558849
3503.227451	344461.966459	48.563853
3503.356832	344456.524435	48.568858
3503.099042	344469.419258	48.573863
3503.586738	344449.666607	48.578868
3503.583296	344464.022978	48.583873
3503.203628	344458.712340	48.588877
3503.703827	344445.219281	48.593882
3503.184767	344462.100709	48.598887
3503.384676	344479.581165	48.603892
3503.550719	344453.872336	48.608897
3503.599978	344472.802009	48.613901
3503.656238	344466.633394	48.618906
3503.578561	344464.940321	48.623911
3503.551880	344464.104606	48.628916
3503.409026	344455.320302	48.633921
3503.349939	344472.714439	48.638925
3503.619728	344452.359901	48.643930
3503.324236	344428.505775	48.648935
3503.289187	344430.267645	48.653940
3503.654281	344426.799183	48.658945
3503.752653	344426.758210	48.663949
3503.462060	344437.061964	48.668954
3503.547939	344437.048421	48.673959
3503.757445	344414.158046	48.678964
3503.554357	344441.196400	48.683969
3503.436404	344437.524318	48.688973
3503.743256	344407.007941	48.693978
3503.317207	344450.549988	48.698983
3503.399527	344425.058011	48.703988
3503.337341	344412.493822	48.708993
3503.398693	344406.171674	48.713997
3503.603176	344395.932503	48.719002
3503.279108	344407.183335	48.724007
3503.596961	344393.388196	48.729012
3503.284996	344400.793629	48.734017
3503.036070	344411.599871	48.739021
3503.518994	344396.556864	48.744026
3503.463564	344398.958295	48.749031
3503.315297	344401.527125	48.754036
3503.525052	344401.570358	48.759041
3503.742704	344402.248681	48.764045
3503.632053	344398.855431	48.769050
3503.114417	344404.129827	48.774055
3503.780636	344396.770269	48.779060
3503.532136	344390.548013	48.784065
3503.530643	344396.911673	48.789069
3503.779775	344401.555775	48.794074
3503.603173	344382.162660	48.799079
3503.436102	344360.299036	48.804084
3503.451629	344366.074576	48.809089
3503.480258	344377.829633	48.814093
3503.835468	344357.207022	48.819098
3503.424523	344365.264447	48.824103
3503.146758	344362.432140	48.829108
3503.471228	344369.482423	48.834113
3503.119975	344376.563174	48.839117
3503.576806	344375.854645	48.844122
3503.349449	344382.330375	48.849127
3503.526666	344372.451860	48.854132
3503.581346	344366.156216	48.859137
3503.542241	344377.845621	48.864141
3503.925638	344383.817537	48.869146
3503.503979	344364.004994	48.874151
3503.577629	344336.528971	48.879156
3503.625610	344342.273929	48.884161
3503.163720	344341.837914	48.889165
3503.366267	344337.682445	48.894170
3503.263555	344346.200213	48.899175
3503.319381	344319.897865	48.904180
3503.666053	344348.122026	48.909185
3503.336465	344336.236436	48.914189
3503.784466	344327.485968	48.919194
3503.594050	344349.813446	48.924199
3503.720537	344344.346416	48.929204
3503.564837	344336.124104	48.934209
3503.751880	344329.629355	48.939213
3503.908421	344312.016207	48.944218
3503.442791	344310.944443	48.949223
3503.501404	344306.251748	48.954228
3503.314016	344313.281146	48.959233
3503.592451	344303.768422	48.964237
3503.815030	344298.871628	48.969242
3503.472635	344307.020038	48.974247
3503.424943	344298.958820	48.979252
3503.359818	344311.008702	48.984257
3503.094190	344319.399510	48.989261
3503.557376	344313.471988	48.994266
3503.701942	344310.852900	48.999271
3503.317040	344294.572573	49.004276
3503.109896	344290.583685	49.009281
3503.487967	344312.184962	49.014285
3503.472001	344293.224587	49.019290
3503.303040	344280.524529	49.024295
3503.494804	344281.996008	49.029300
3503.588365	344262.152885	49.034305
3503.159943	344292.281365	49.039309
3503.555755	344274.401296	49.044314
3503.164398	344288.691770	49.049319
3503.295135	344279.304206	49.054324
3503.267900	344279.308545	49.059329
3503.539513	344280.131060	49.064333
3503.428211	344279.614164	49.069338
3503.507634	344287.492260	49.074343
3503.669628	344285.557662	49.079348
3503.795669	344284.545078	49.084353
3503.535442	344291.051469	49.089357
3503.462861	344286.048617	49.094362
3503.449492	344284.574454	49.099367
3503.699900	344282.244074	49.104372
3503.697549	344272.266664	49.109377
3503.138028	344269.809794	49.114381
3503.485020	344246.515814	49.119386
3503.233792	344253.249869	49.124391
3502.999235	344246.694497	49.129396
3503.297166	344280.093482	49.134401
3503.360504	344267.611231	49.139405
3503.528081	344271.708257	49.144410
3503.067565	344282.420706	49.149415
3503.407598	344282.901507	49.154420
3503.632702	344268.510115	49.159425
3503.549320	344261.599947	49.164429
3503.386788	344268.141802	49.169434
3503.197101	344240.223748	49.174439
3503.480515	344275.457692	49.179444
3503.732615	344245.993486	49.184449
3503.542165	344258.292275	49.189453
3503.493200	344254.049295	49.194458
3503.485943	344266.624564	49.199463
3503.583927	344244.489910	49.204468
3503.534744	344250.657496	49.209473
3503.359627	344276.266100	49.214477
3503.403482	344256.761730	49.219482
3503.360898	344253.561340	49.224487
3503.470805	344277.623119	49.229492
3503.124134	344260.751306	49.234497
3503.041774	344268.044094	49.239501
3503.576627	344258.745360	49.244506
3503.435710	344264.036571	49.249511
3503.213138	344276.493156	49.254516
3503.652856	344265.173174	49.259521
3503.210852	344266.108510	49.264525
3503.426294	344268.874380	49.269530
3503.528882	344237.244796	49.274535
3503.446582	344265.867713	49.279540
3503.681241	344245.187761	49.284545
3503.808534	344246.058547	49.289549
3503.606246	344229.672971	49.294554
3503.392945	344248.873308	49.299559
3503.735380	344230.594407	49.304564
3503.735698	344260.044234	49.309569
3503.494099	344233.916137	49.314573
3503.780352	344232.089161	49.319578
3503.410077	344225.147985	49.324583
3503.547992	344206.774141	49.329588
3503.416884	344202.875042	49.334593
3503.471758	344210.146141	49.339597
3503.615566	344180.953560	49.344602
3503.433337	344200.327176	49.349607
3503.678008	344187.790787	49.354612
3503.672819	344222.434049	49.359617
3503.529682	344183.207193	49.364621
3503.771398	344217.989598	49.369626
3503.505385	344188.530914	49.374631
3503.123487	344180.929775	49.379636
3503.190395	344159.258168	49.384641
3503.324074	344188.254236	49.389645
3503.514497	344183.566146	49.394650
3503.331104	344190.213122	49.399655
3503.367839	344170.786210	49.404660
3503.534344	344158.236719	49.409665
3503.031902	344154.981757	49.414669
3503.722883	344156.094325	49.419674
3503.362221	344172.390813	49.424679
3503.351741	344169.058074	49.429684
3503.587867	344158.126610	49.434689
3503.480800	344176.393844	49.439693
3503.805727	344159.441278	49.444698
3503.500028	344159.871446	49.449703
3503.474125	344169.827956	49.454708
3503.506148	344171.401053	49.459713
3503.446467	344170.163293	49.464717
3503.735378	344166.197787	49.469722
3503.317922	344162.700307	49.474727
3503.618683	344147.711490	49.479732
3503.116761	344138.627555	49.484737
3502.905948	344156.580299	49.489741
3503.444261	344139.517631	49.494746
3503.216192	344188.653832	49.499751
3503.584678	344149.804234	49.504756
3503.702940	344168.137661	49.509761
3503.400404	344148.026224	49.514765
3503.150402	344145.342239	49.519770
3503.433402	344134.581536	49.524775
3503.392779	344123.999263	49.529780
3503.489698	344152.619354	49.534785
3503.222847	344144.592763	49.539789
3503.461594	344132.210021	49.544794
3503.011400	344146.815274	49.549799
3503.349685	344157.503273	49.554804
3503.629724	344134.219834	49.559809
3503.355363	344160.251438	49.564813
3503.504922	344134.315993	49.569818
3503.579074	344154.590877	49.574823
3503.952969	344151.019193	49.579828
3503.723342	344140.772248	49.584833
3503.559495	344147.416139	49.589837
3503.903783	344135.780322	49.594842
3503.681500	344142.128008	49.599847
3503.797228	344120.830474	49.604852
3503.664292	344114.029938	49.609857
3503.409077	344117.353844	49.614861
3503.388864	344111.757263	49.619866
3503.338463	344121.030405	49.624871
3503.560088	344109.388522	49.629876
3503.592196	344118.394082	49.634881
3503.495105	344129.736352	49.639885
3503.702002	344108.908020	49.644890
3503.551515	344084.598118	49.649895
3503.639482	344093.391221	49.654900
3503.587164	344080.367235	49.659905
3503.267948	344062.218340	49.664909
3503.420597	344087.673392	49.669914
3503.887277	344053.771678	49.674919
3503.492119	344089.571179	49.679924
3503.704276	344070.854658	49.684929
3503.394155	344081.136107	49.689933
3503.724812	344075.662227	49.694938
3503.254853	344075.482023	49.699943
3503.202406	344087.224501	49.704948
3503.802894	344086.213267	49.709953
3503.482975	344055.897614	49.714957
3503.386715	344057.160098	49.719962
3503.239002	344061.408799	49.724967
3503.285092	344038.518662	49.729972
3503.379154	344046.267206	49.734977
3502.885009	344056.272309	49.739981
3503.420028	344044.199061	49.744986
3503.397258	344048.148019	49.749991
3503.481251	344049.102014	49.754996
3503.600003	344038.341807	49.760001
3503.523529	344046.168221	49.765005
3503.360148	344045.175936	49.770010
3503.456746	344049.080569	49.775015
3503.488269	344048.261100	49.780020
3503.451020	344045.798012	49.785025
3503.467644	344059.362244	49.790029
3503.725105	344054.536277	49.795034
3503.239502	344050.336859	49.800039
3503.261092	344075.278109	49.805044
3503.774290	344060.357500	49.810049
3503.496563	344049.278171	49.815053
3503.748686	344046.871150	49.820058
3503.553000	344028.040918	49.825063
3503.711865	344026.437705	49.830068
3503.779609	344021.768997	49.835073
3503.492675	344024.639757	49.840077
3503.849309	344015.089170	49.845082
3503.504561	344019.241756	49.850087
3503.509831	344024.178978	49.855092
3503.536427	344028.934652	49.860097
3503.531172	344012.645135	49.865101
3503.374852	344010.404500	49.870106
3503.638652	344015.504480	49.875111
3503.741778	343993.139836	49.880116
3503.728968	343997.749020	49.885121
3503.351716	343999.488642	49.890125
3503.562546	343997.902667	49.895130
3503.271832	344011.540952	49.900135
3503.230332	344007.958571	49.905140
3503.315189	343998.781846	49.910145
3503.559519	343992.430726	49.915149
3503.380188	343993.553622	49.920154
3503.432210	344004.515989	49.925159
3503.750547	343998.178623	49.930164
3503.734871	343993.268565	49.935169
3503.201512	343983.935038	49.940173
3503.634482	343971.496103	49.945178
3503.293428	343965.644787	49.950183
3503.262164	343966.082477	49.955188
3503.570255	343972.117247	49.960193
3503.258151	343965.243205	49.965197
3503.668959	343956.142211	49.970202
3503.516769	343975.994772	49.975207
3503.418299	343961.705369	49.980212
3503.394752	343957.381988	49.985217
3503.232829	343964.891023	49.990221
3503.463226	343972.719838	49.995226
3503.502204	343961.234071	50.000231
3503.450214	343961.573222	50.005236
3503.543705	343967.667374	50.010241
3503.389682	343960.055634	50.015245
3503.288954	343968.089522	50.020250
3503.420128	343970.639646	50.025255
3503.710022	343966.444888	50.030260
3503.507666	343957.720824	50.035265
3503.108426	343971.987166	50.040269
3503.429362	343967.380240	50.045274
3503.183039	343959.121295	50.050279
3503.358462	343958.889965	50.055284
3503.578711	343964.455002	50.060289
3503.621054	343969.920896	50.065293
3503.632661	343944.465346	50.070298
3503.484914	343938.685282	50.075303
3503.669074	343932.776382	50.080308
3503.699400	343926.840895	50.085313
3503.653539	343933.644333	50.090317
3503.941917	343922.297305	50.095322
3503.719920	343938.291942	50.100327
3503.291215	343910.258799	50.105332
3503.636489	343907.837045	50.110337
3503.113456	343899.240032	50.115341
3503.404559	343898.252253	50.120346
3503.328282	343906.409553	50.125351
3503.422075	343904.485725	50.130356
3503.582485	343898.020594	50.135361
3503.585927	343907.616155	50.140365
3503.484311	343896.203510	50.145370
3503.331474	343905.696510	50.150375
3503.461278	343898.981680	50.155380
3503.368000	343899.505536	50.160385
3503.261685	343904.664039	50.165389
3503.168685	343898.468055	50.170394
3503.368085	343904.749100	50.175399
3503.441769	343899.901267	50.180404
3503.495694	343909.870653	50.185409
3503.370371	343911.697718	50.190413
3503.487539	343893.887041	50.195418
3503.336882	343905.746897	50.200423
3503.609398	343908.351039	50.205428
3503.349915	343910.581119	50.210433
3503.244910	343906.194252	50.215437
3503.466972	343911.529923	50.220442
3503.304276	343910.130267	50.225447
3503.351546	343897.421396	50.230452
3503.721980	343929.332797	50.235457
3503.501566	343904.499347	50.240461
3503.357313	343883.344645	50.245466
3503.465618	343877.702270	50.250471
3503.564448	343876.337629	50.255476
3503.524527	343890.521729	50.260481
3503.408886	343892.169087	50.265485
3503.573349	343878.932608	50.270490
3503.468912	343899.515805	50.275495
3503.541477	343869.901620	50.280500
3503.570989	343891.659971	50.285505
3503.468861	343887.323554	50.290509
3503.397594	343879.698721	50.295514
3503.418474	343903.825633	50.300519
3503.514102	343895.970786	50.305524
3503.903996	343890.207533	50.310529
3503.187657	343855.703670	50.315533
3503.497088	343855.298430	50.320538
3503.697198	343852.314187	50.325543
3503.511650	343847.736418	50.330548
3503.725739	343836.172035	50.335553
3503.697563	343845.161713	50.340557
3503.875037	343844.344621	50.345562
3503.227661	343845.846961	50.350567
3503.289319	343843.470044	50.355572
3503.353312	343847.634383	50.360577
3503.400747	343855.466685	50.365581
3503.563561	343860.480829	50.370586
3503.370262	343843.075574	50.375591
3503.291628	343837.793649	50.380596
3503.581092	343820.388425	50.385601
3503.557075	343824.337595	50.390605
3503.674651	343812.839373	50.395610
3503.611584	343797.831627	50.400615
3503.781766	343825.702132	50.405620
3503.718652	343807.614486	50.410625
3503.433219	343825.222773	50.415629
3503.719411	343802.065501	50.420634
3503.377307	343826.784362	50.425639
3503.625218	343771.535874	50.430644
3503.829185	343791.688543	50.435649
3503.459911	343784.492619	50.440653
3503.567321	343765.716201	50.445658
3503.611408	343779.250700	50.450663
3503.504005	343790.467396	50.455668
3503.677655	343784.101974	50.460673
3503.236084	343772.412151	50.465677
3503.417964	343786.968472	50.470682
3503.283227	343788.567943	50.475687
3503.443678	343768.179550	50.480692
3503.465049	343788.411996	50.485697
3503.188818	343787.666632	50.490701
3503.416497	343783.863504	50.495706
3503.566107	343788.090673	50.500711
3503.659219	343773.338222	50.505716
3503.167576	343759.390922	50.510721
3502.788748	343768.563318	50.515725
3503.152685	343776.294686	50.520730
3503.322865	343768.886204	50.525735
3503.232893	343747.391973	50.530740
3503.240983	343717.813360	50.535745
3502.822046	343707.112646	50.540749
3503.161856	343642.406129	50.545754
3502.715211	343585.485505	50.550759
3502.465435	343520.719345	50.555764
3502.283365	343462.993157	50.560769
3502.133979	343385.356729	50.565773
3501.952026	343289.652988	50.570778
3501.505473	343209.288824	50.575783
3501.235175	343108.838852	50.580788
3500.922172	343011.984500	50.585793
3500.231069	342903.989924	50.590797
3500.338269	342790.396283	50.595802
3499.532669	342658.696013	50.600807
3499.166333	342563.274815	50.605812
3499.217071	342423.089624	50.610817
3498.285567	342298.204801	50.615821
3497.732183	342171.198127	50.620826
3497.060094	342045.762684	50.625831
3496.980990	341913.309581	50.630836
3496.351280	341771.550471	50.635841
3495.946086	341638.002869	50.640845
3495.633509	341476.898258	50.645850
3494.870408	341329.991899	50.650855
3494.596397	341182.906046	50.655860
3494.072100	341019.415502	50.660865
3493.278766	340863.527211	50.665869
3492.942366	340696.951509	50.670874
3492.280683	340541.932530	50.675879
3491.495998	340370.437619	50.680884
3490.814280	340230.668726	50.685889
3490.256158	340064.279131	50.690893
3490.165321	339887.251214	50.695898
3489.292529	339721.394119	50.700903
3488.562122	339559.663338	50.705908
3488.311188	339387.088606	50.710913
3487.261823	339209.090297	50.715917
3486.777757	339034.464104	50.720922
3486.119768	338875.163895	50.725927
3485.648488	338694.399898	50.730932
3485.067297	338522.689645	50.735937
3484.139223	338352.459318	50.740941
3483.856327	338166.598308	50.745946
3483.046581	337994.108196	50.750951
3482.390504	337813.676436	50.755956
3481.794448	337631.758222	50.760961
3480.987798	337470.976150	50.765965
3480.507691	337291.024258	50.770970
3480.048314	337110.534012	50.775975
3479.562001	336929.283833	50.780980
3478.915562	336741.210633	50.785985
3478.108766	336556.115237	50.790989
3477.504641	336363.783006	50.795994
3476.506022	336192.820006	50.800999
3475.834476	336001.872068	50.806004
3475.582285	335812.359250	50.811009
3474.550436	335639.490823	50.816013
3474.356533	335448.593089	50.821018
3473.486091	335276.207360	50.826023
3472.776356	335066.933623	50.831028
3472.054251	334897.196502	50.836033
3471.298447	334716.797625	50.841037
3470.753229	334525.341883	50.846042
3470.170154	334337.710231	50.851047
3469.231913	334155.353042	50.856052
3468.749736	333985.550287	50.861057
3467.938139	333796.502217	50.866061
3467.408275	333607.001765	50.871066
3466.604649	333423.526694	50.876071
3465.881974	333236.448771	50.881076
3465.485145	333046.314784	50.886081
3464.413984	332870.161575	50.891085
3464.206248	332680.734995	50.896090
3463.700579	332499.323447	50.901095
3462.874903	332312.768544	50.906100
3462.146160	332129.252833	50.911105
3461.155879	331936.409303	50.916109
3460.635039	331748.404524	50.921114
3459.996821	331562.530877	50.926119
3459.185627	331378.007955	50.931124
3458.487261	331205.814192	50.936129
3457.495915	331032.266117	50.941133
3457.140906	330852.506902	50.946138
3456.533993	330668.357234	50.951143
3455.806592	330494.206062	50.956148
3455.484767	330313.931111	50.961153
3454.623704	330119.993092	50.966157
3453.964990	329926.811807	50.971162
3453.199466	329744.950795	50.976167
3452.703055	329562.817658	50.981172
3451.995197	329379.877358	50.986177
3451.200760	329202.169476	50.991181
3450.470832	329014.267205	50.996186
3449.761768	328839.472812	51.001191
3449.035008	328661.269238	51.006196
3448.477298	328457.426142	51.011201
3447.931876	328301.724824	51.016205
3447.159175	328118.206183	51.021210
3446.211412	327925.371044	51.026215
3445.977555	327751.033699	51.031220
3445.314465	327563.932039	51.036225
3444.232021	327390.670087	51.041229
3443.871888	327192.928289	51.046234
3442.884152	327014.100244	51.051239
3442.189408	326827.129139	51.056244
3441.765043	326642.966384	51.061249
3441.118739	326470.142657	51.066253
3440.703960	326278.390385	51.071258
3439.754263	326106.199434	51.076263
3439.082006	325918.560679	51.081268
3438.400157	325729.089849	51.086273
3437.440948	325550.559554	51.091277
3437.254585	325369.156915	51.096282
3436.422496	325201.426516	51.101287
3435.962903	325020.931973	51.106292
3435.323966	324829.440875	51.111297
3434.527935	324654.956553	51.116301
3434.112826	324462.487163	51.121306
3432.980010	324280.697110	51.126311
3432.336730	324103.997838	51.131316
3431.709053	323908.072626	51.136321
3430.776727	323742.417478	51.141325
3430.299775	323563.704804	51.146330
3429.599345	323379.171011	51.151335
3428.692329	323198.488676	51.156340
3428.280580	323030.560153	51.161345
3427.691070	322845.472979	51.166349
3427.138551	322665.420923	51.171354
3426.319814	322492.056037	51.176359
3425.715784	322325.837005	51.181364
3425.091546	322143.019898	51.186369
3424.062294	321958.076752	51.191373
3424.015696	321773.996298	51.196378
3423.150710	321597.072312	51.201383
3422.253517	321417.326806	51.206388
3421.909761	321225.118962	51.211393
3420.809978	321060.198105	51.216397
3420.262160	320867.410674	51.221402
3419.442234	320695.290082	51.226407
3418.596705	320522.307501	51.231412
3418.208986	320338.176180	51.236417
3417.297057	320172.001812	51.241421
3417.079941	319991.305666	51.246426
3416.256859	319817.707104	51.251431
3415.640317	319642.827901	51.256436
3415.086754	319453.119323	51.261441
3414.246670	319278.860416	51.266445
3413.742924	319104.344297	51.271450
3412.919955	318936.905979	51.276455
3411.965126	318746.393693	51.281460
3411.654276	318565.454971	51.286465
3411.018900	318394.599501	51.291469
3410.410796	318208.869204	51.296474
3409.764834	318047.766993	51.301479
3408.957824	317856.822145	51.306484
3408.427827	317677.418698	51.311489
3407.828892	317494.817498	51.316493
3407.112115	317313.864216	51.321498
3406.019914	317145.217654	51.326503
3405.295436	316966.505688	51.331508
3405.108687	316783.914366	51.336513
3404.050653	316612.002215	51.341517
3403.501933	316432.675837	51.346522
3402.748202	316263.057570	51.351527
3401.867790	316090.861798	51.356532
3401.358089	315921.051582	51.361537
3400.602175	315754.131907	51.366541
3400.189177	315571.268590	51.371546
3399.588306	315398.594555	51.376551
3398.558508	315224.893130	51.381556
3398.539368	315042.068435	51.386561
3397.579681	314880.501429	51.391565
3396.733655	314698.443478	51.396570
3396.069911	314523.486198	51.401575
3395.144867	314350.377867	51.406580
3394.635266	314180.462906	51.411585
3394.056338	314004.803828	51.416589
3393.434788	313828.259965	51.421594
3392.612693	313655.312461	51.426599
3391.843634	313492.032562	51.431604
3391.489561	313315.623800	51.436609
3390.923570	313132.347530	51.441613
3390.351593	312965.699889	51.446618
3389.868229	312808.943488	51.451623
3389.195811	312608.163908	51.456628
3388.579750	312428.382953	51.461633
3387.698251	312256.741286	51.466637
3387.378342	312067.618490	51.471642
3386.240097	311901.033325	51.476647
3385.571662	311713.136401	51.481652
3384.975296	311538.163645	51.486657
3384.409939	311368.456837	51.491661
3383.606850	311187.583035	51.496666
3382.954407	311012.618338	51.501671
3382.219053	310833.617633	51.506676
3381.363396	310657.513168	51.511681
3380.204124	310501.471593	51.516685
3380.082250	310323.900954	51.521690
3379.237955	310155.153199	51.526695
3378.531720	309976.757724	51.531700
3378.076071	309805.783509	51.536705
3377.192556	309630.394919	51.541709
3376.646453	309469.340311	51.546714
3376.153843	309306.545420	51.551719
3375.291603	309134.819674	51.556724
3375.161726	308959.947541	51.561729
3373.968005	308790.107203	51.566733
3373.276463	308611.529125	51.571738
3372.752271	308438.704875	51.576743
3372.001856	308267.520457	51.581748
3371.395578	308099.496142	51.586753
3370.761499	307932.061695	51.591757
3369.881124	307757.663065	51.596762
3369.272474	307590.733445	51.601767
3368.744312	307413.884914	51.606772
3368.531162	307243.734605	51.611777
3367.435525	307077.059588	51.616781
3366.721713	306900.188779	51.621786
3366.269913	306728.496685	51.626791
3365.347795	306552.575100	51.631796
3364.818486	306376.234640	51.636801
3364.239323	306211.870584	51.641805
3363.603457	306031.472047	51.646810
3362.722035	305862.520647	51.651815
3361.798176	305694.314247	51.656820
3361.855096	305514.620344	51.661825
3360.671731	305355.724032	51.666829
3360.237324	305181.633431	51.671834
3359.580853	305002.280871	51.676839
3358.859496	304836.919008	51.681844
3358.082569	304666.396194	51.686849
3357.155228	304502.263400	51.691853
3356.824807	304314.123633	51.696858
3355.724824	304152.309658	51.701863
3355.351283	303984.829051	51.706868
3354.610992	303819.876442	51.711873
3354.000151	303648.842285	51.716877
3353.282149	303470.898139	51.721882
3352.648517	303306.717521	51.726887
3351.923554	303134.300181	51.731892
3351.589625	302972.898514	51.736897
3350.642527	302802.909727	51.741901
3350.340200	302633.277158	51.746906
3349.244109	302468.175577	51.751911
3348.429994	302300.609935	51.756916
3348.099462	302124.640187	51.761921
3347.277849	301960.895283	51.766925
3346.686328	301787.080121	51.771930
3346.049556	301625.826783	51.776935
3345.374916	301448.331781	51.781940
3344.744520	301284.352191	51.786945
3343.874427	301111.038731	51.791949
3343.174982	300939.684468	51.796954
3342.316587	300787.047490	51.801959
3341.736800	300611.853994	51.806964
3341.355376	300448.216165	51.811969
3340.521841	300294.428802	51.816973
3340.168847	300133.027211	51.821978
3339.550261	299943.017639	51.826983
3338.490969	299790.895372	51.831988
3337.775870	299618.141543	51.836993
3337.181867	299456.344485	51.841997
3336.750360	299294.368772	51.847002
3335.851484	299119.453375	51.852007
3334.993615	298955.405580	51.857012
3335.262669	298785.907785	51.862017
3334.105735	298625.115785	51.867021
3333.758345	298459.662516	51.872026
3332.987355	298291.729415	51.877031
3332.073886	298113.173576	51.882036
3331.868368	297939.777216	51.887041
3330.569377	297779.719995	51.892045
3329.964661	297597.091053	51.897050
3329.330541	297436.368101	51.902055
3328.603822	297272.501759	51.907060
3328.224517	297105.728028	51.912065
3327.171192	296936.539531	51.917069
3326.479361	296763.244458	51.922074
3325.828969	296612.735632	51.927079
3325.423065	296447.901024	51.932084
3324.725739	296273.511298	51.937089
3323.988072	296115.579517	51.942093
3323.472674	295937.977336	51.947098
3322.760430	295771.738992	51.952103
3322.167998	295621.525846	51.957108
3321.637632	295434.528219	51.962113
3321.019535	295270.362878	51.967117
3320.140625	295098.725840	51.972122
3319.573482	294930.350083	51.977127
3318.932395	294767.690546	51.982132
3318.395766	294585.175377	51.987137
3317.275001	294429.594946	51.992141
3316.757610	294245.624810	51.997146
3316.004572	294095.334104	52.002151
3315.338336	293918.594482	52.007156
3314.936811	293757.882743	52.012161
3314.046120	293586.551970	52.017165
3313.084234	293418.670424	52.022170
3312.791216	293264.053341	52.027175
3312.093766	293098.778342	52.032180
3311.756084	292919.362826	52.037185
3310.788015	292754.588802	52.042189
3310.271273	292593.588861	52.047194
3309.727618	292423.042760	52.052199
3308.719006	292256.186470	52.057204
3308.052977	292086.117902	52.062209
3307.165512	291923.189688	52.067213
3306.768643	291749.181779	52.072218
3305.700088	291593.922262	52.077223
3305.191628	291424.184865	52.082228
3304.624611	291264.541791	52.087233
3303.496210	291108.145403	52.092237
3303.350573	290939.114325	52.097242
3302.600577	290778.684932	52.102247
3301.720665	290613.182458	52.107252
3301.271825	290450.642351	52.112257
3300.561034	290294.994394	52.117261
3300.193878	290132.619450	52.122266
3299.081417	289971.635692	52.127271
3298.648329	289811.664958	52.132276
3298.149042	289639.403676	52.137281
3297.109915	289496.286416	52.142285
3296.530437	289327.908736	52.147290
3296.028460	289154.705284	52.152295
3295.188108	289001.674833	52.157300
3294.608955	288833.449628	52.162305
3294.086217	288680.394242	52.167309
3293.242140	288517.304338	52.172314
3292.429680	288355.380870	52.177319
3291.700440	288198.206650	52.182324
3290.972072	288044.750527	52.187329
3290.537243	287882.436002	52.192333
3290.364024	287720.640308	52.197338
3289.705437	287560.220178	52.202343
3288.437261	287398.190047	52.207348
3288.159704	287230.323784	52.212353
3287.385907	287080.949278	52.217357
3286.673236	286905.638636	52.222362
3286.170422	286743.206984	52.227367
3285.313349	286580.398342	52.232372
3284.764724	286411.912403	52.237377
3283.758397	286266.445482	52.242381
3283.491391	286091.420505	52.247386
3282.755358	285933.304021	52.252391
3281.840027	285778.297471	52.257396
3281.403064	285599.147863	52.262401
3280.483898	285449.337278	52.267405
3280.343124	285290.617015	52.272410
3279.605460	285135.633050	52.277415
3278.783191	284960.415265	52.282420
3278.649530	284789.036038	52.287425
3277.606118	284628.140715	52.292429
3276.786233	284463.797245	52.297434
3276.175926	284302.043781	52.302439
3275.480766	284138.673721	52.307444
3274.920689	283975.664258	52.312449
3273.815838	283823.004591	52.317453
3273.446624	283641.882420	52.322458
3272.348739	283500.070996	52.327463
3271.871167	283333.457254	52.332468
3271.411979	283172.952920	52.337473
3270.632555	283014.663993	52.342477
3270.253003	282856.770191	52.347482
3269.694571	282686.909106	52.352487
3268.849980	282527.382405	52.357492
3268.181652	282365.561102	52.362497
3267.276946	282200.287999	52.367501
3266.699266	282038.859760	52.372506
3266.280276	281887.288061	52.377511
3265.483318	281719.145339	52.382516
3265.129030	281548.156503	52.387521
3264.338339	281394.427751	52.392525
3263.485732	281233.272018	52.397530
3262.811485	281064.116458	52.402535
3262.074168	280898.714675	52.407540
3261.448688	280742.463753	52.412545
3260.604800	280577.562658	52.417549
3260.240245	280419.640422	52.422554
3259.389338	280263.501473	52.427559
3258.533079	280090.325032	52.432564
3258.194956	279939.529657	52.437569
3257.490554	279780.897017	52.442573
3256.695746	279615.249391	52.447578
3256.082210	279459.811334	52.452583
3255.323772	279290.006561	52.457588
3254.688214	279138.392191	52.462593
3253.951486	278976.580996	52.467597
3253.560415	278819.885172	52.472602
3252.867370	278658.550921	52.477607
3252.060572	278507.345586	52.482612
3251.278443	278332.603560	52.487617
3250.373124	278189.207096	52.492621
3249.966071	278033.481505	52.497626
3249.293890	277861.319805	52.502631
3248.631725	277709.200115	52.507636
3248.106619	277560.063997	52.512641
3246.969650	277410.540766	52.517645
3246.797958	277250.346375	52.522650
3246.140010	277081.798863	52.527655
3245.166934	276938.005528	52.532660
3244.697302	276769.606482	52.537665
3243.790821	276622.389832	52.542669
3243.137096	276463.188515	52.547674
3242.485654	276315.625884	52.552679
3242.097683	276168.760150	52.557684
3241.182852	276009.701998	52.562689
3240.395828	275863.867187	52.567693
3239.909813	275693.917123	52.572698
3239.006101	275531.240693	52.577703
3238.717752	275393.782491	52.582708
3238.088561	275226.376446	52.587713
3237.513057	275073.198740	52.592717
3237.057239	274914.730144	52.597722
3236.216608	274760.881273	52.602727
3235.477216	274596.370602	52.607732
3234.792365	274439.135268	52.612737
3233.934160	274278.616474	52.617741
3233.709933	274125.128537	52.622746
3232.938369	273964.748862	52.627751
3232.047589	273802.681675	52.632756
3231.629668	273639.011586	52.637761
3230.658296	273492.187264	52.642765
3230.116008	273329.606546	52.647770
3229.362060	273179.666175	52.652775
3228.400221	273016.540620	52.657780
3227.912643	272865.386588	52.662785
3227.323519	272709.664330	52.667789
3227.040316	272558.172374	52.672794
3225.894815	272396.731385	52.677799
3225.306813	272243.097407	52.682804
3224.803120	272089.348234	52.687809
3224.300305	271936.159246	52.692813
3223.701156	271778.681368	52.697818
3223.045018	271616.399010	52.702823
3222.141274	271463.400860	52.707828
3221.782208	271306.801927	52.712833
3220.759339	271148.856346	52.717837
3220.752973	270990.342474	52.722842
3219.587112	270831.553646	52.727847
3218.620894	270667.639596	52.732852
3218.077175	270518.634104	52.737857
3217.186928	270357.815230	52.742861
3217.050066	270202.149132	52.747866
3216.171901	270042.525421	52.752871
3215.290672	269888.810873	52.757876
3214.635446	269728.362440	52.762881
3213.756463	269581.320295	52.767885
3213.341498	269434.026488	52.772890
3212.597990	269263.404817	52.777895
3211.934183	269126.668847	52.782900
3211.701599	268968.955233	52.787905
3210.752868	268821.389459	52.792909
3210.207545	268660.414531	52.797914
3209.182717	268514.388966	52.802919
3208.551168	268345.150585	52.807924
3208.361909	268193.466292	52.812929
3207.408127	268049.823618	52.817933
3206.767860	267898.210762	52.822938
3206.096330	267740.541462	52.827943
3205.352305	267593.402045	52.832948
3204.927527	267430.854838	52.837953
3203.944918	267284.415431	52.842957
3203.524489	267130.374007	52.847962
3202.709457	266974.561356	52.852967
3202.111070	266807.304742	52.857972
3201.826890	266664.320559	52.862977
3200.521359	266507.490539	52.867981
3199.829155	266351.658661	52.872986
3199.165406	266203.004348	52.877991
3198.690672	266061.502188	52.882996
3198.281437	265906.873633	52.888001
3197.460402	265747.012925	52.893005
3196.854638	265597.891219	52.898010
3196.022486	265442.947728	52.903015
3194.966269	265292.496661	52.908020
3194.685616	265142.941660	52.913025
3193.842968	264992.609723	52.918029
3193.266471	264844.425984	52.923034
3192.779888	264700.175621	52.928039
3191.925700	264552.265144	52.933044
3191.439470	264392.402943	52.938049
3190.326688	264261.724409	52.943053
3189.885804	264105.446147	52.948058
3189.179730	263958.785874	52.953063
3188.532194	263811.428764	52.958068
3187.885932	263657.118761	52.963073
3187.020670	263515.984941	52.968077
3186.602359	263362.606784	52.973082
3186.128275	263229.000634	52.978087
3185.494522	263072.727886	52.983092
3184.855510	262922.542873	52.988097
3184.083237	262772.531822	52.993101
3183.471915	262623.768769	52.998106
3182.781225	262462.029728	53.003111
3181.957418	262326.645600	53.008116
3181.547822	262155.693812	53.013121
3180.721980	262007.066866	53.018125
3180.225006	261857.904068	53.023130
3179.610337	261712.987622	53.028135
3178.814067	261563.566714	53.033140
3178.341103	261405.690358	53.038145
3177.470383	261262.877539	53.043149
3176.600926	261104.962213	53.048154
3176.197767	260967.652998	53.053159
3175.466003	260804.113148	53.058164
3174.461694	260652.586345	53.063169
3173.900065	260523.503028	53.068173
3173.430709	260363.334589	53.073178
3172.861782	260213.267200	53.078183
3171.961790	260065.849981	53.083188
3171.525796	259909.191072	53.088193
3170.640906	259774.097966	53.093197
3170.361197	259603.738392	53.098202
3169.761830	259470.281128	53.103207
3168.634624	259305.200310	53.108212
3168.386184	259169.166385	53.113217
3167.606143	259014.752672	53.118221
3166.753878	258862.948172	53.123226
3165.948363	258718.241808	53.128231
3165.433144	258572.318090	53.133236
3165.048839	258421.585855	53.138241
3164.318383	258278.166719	53.143245
3163.654280	258115.280029	53.148250
3162.835810	257970.754438	53.153255
3162.303807	257825.776129	53.158260
3161.922718	257661.393328	53.163265
3160.788724	257520.534319	53.168269
3160.455844	257362.918431	53.173274
3159.566476	257213.998679	53.178279
3158.867730	257056.517302	53.183284
3158.308516	256906.297613	53.188289
3157.417082	256766.190183	53.193293
3156.986779	256612.308471	53.198298
3156.311893	256465.825613	53.203303
3155.393771	256320.934846	53.208308
3154.789624	256167.819511	53.213313
3154.143263	256033.429375	53.218317
3153.732423	255882.753978	53.223322
3152.855496	255728.255964	53.228327
3152.257305	255586.243805	53.233332
3151.527150	255428.666730	53.238337
3150.547281	255291.935937	53.243341
3150.370632	255137.047418	53.248346
3149.496308	254978.016414	53.253351
3148.948765	254837.830395	53.258356
3148.002485	254677.257527	53.263361
3147.216052	254540.904113	53.268365
3146.652760	254396.951779	53.273370
3146.025149	254244.274550	53.278375
3145.392370	254106.343639	53.283380
3144.936836	253963.749794	53.288385
3143.689652	253818.709168	53.293389
3143.290469	253676.819695	53.298394
3142.887651	253537.299327	53.303399
3141.795409	253388.108878	53.308404
3141.472173	253240.477670	53.313409
3140.651950	253095.701113	53.318413
3140.292085	252952.685432	53.323418
3139.509367	252810.780917	53.328423
3138.444335	252668.157185	53.333428
3138.374130	252512.235291	53.338433
3137.260915	252381.690657	53.343437
3136.957010	252223.641325	53.348442
3136.151949	252087.980268	53.353447
3135.143663	251944.864273	53.358452
3134.843575	251783.554999	53.363457
3133.850986	251658.136083	53.368461
3133.224504	251517.048286	53.373466
3132.328978	251372.743459	53.378471
3132.076447	251232.997384	53.383476
3131.614247	251090.534216	53.388481
3130.458824	250958.698549	53.393485
3130.127297	250805.468070	53.398490
3129.608828	250666.604946	53.403495
3128.705417	250526.122071	53.408500
3128.169180	250380.895385	53.413505
3127.625124	250244.379581	53.418509
3127.041200	250086.605760	53.423514
3126.052910	249952.885407	53.428519
3125.464483	249804.458735	53.433524
3124.800492	249656.196958	53.438529
3123.928070	249513.418093	53.443533
3123.458704	249371.186763	53.448538
3122.785293	249227.790940	53.453543
3122.453975	249089.357959	53.458548
3121.339665	248950.641553	53.463553
3120.795809	248808.218798	53.468557
3120.332165	248671.156841	53.473562
3119.484642	248518.341284	53.478567
3118.451447	248367.949080	53.483572
3118.178101	248234.040667	53.488577
3117.416220	248092.824527	53.493581
3116.911268	247949.275916	53.498586
3116.019678	247793.539476	53.503591
3115.649586	247668.661852	53.508596
3114.802662	247517.502515	53.513601
3113.856711	247376.316190	53.518605
3113.731732	247236.222443	53.523610
3112.857978	247089.931787	53.528615
3112.019942	246961.767327	53.533620
3111.547325	246804.437689	53.538625
3110.689493	246672.991527	53.543629
3110.148941	246541.342480	53.548634
3109.703741	246392.107083	53.553639
3108.959148	246248.649019	53.558644
3108.408913	246099.023105	53.563649
3107.541259	245964.905260	53.568653
3107.097772	245821.883831	53.573658
3106.466475	245671.354443	53.578663
3105.855166	245524.463640	53.583668
3104.990007	245389.734787	53.588673
3104.292034	245239.751205	53.593677
3103.482603	245105.395799	53.598682
3102.772516	244949.913902	53.603687
3101.899473	244822.138947	53.608692
3101.583839	244672.604798	53.613697
3100.800634	244539.366291	53.618701
3100.222509	244393.744744	53.623706
3099.504507	244257.822336	53.628711
3098.452971	244117.267232	53.633716
3098.017766	243977.455093	53.638721
3097.349200	243836.992474	53.643725
3097.233445	243697.410198	53.648730
3096.340560	243563.960859	53.653735
3095.428506	243416.228713	53.658740
3094.837568	243271.221621	53.663745
3094.047011	243147.305965	53.668749
3093.455750	242996.518650	53.673754
3092.976308	242856.561947	53.678759
3092.216025	242728.873079	53.683764
3091.745395	242588.762491	53.688769
3090.720131	242447.441124	53.693773
3090.031160	242305.302747	53.698778
3089.745099	242168.168291	53.703783
3089.132168	242028.895737	53.708788
3088.314918	241886.447103	53.713793
3087.405785	241748.826037	53.718797
3087.199609	241601.824673	53.723802
3086.325493	241452.611904	53.728807
3085.736996	241321.561427	53.733812
3085.243751	241174.937060	53.738817
3084.359621	241030.870281	53.743821
3083.784311	240887.391416	53.748826
3082.915830	240752.286067	53.753831
3082.189474	240609.086093	53.758836
3081.568040	240466.429910	53.763841
3080.714767	240327.146452	53.768845
3080.130484	240184.102766	53.773850
3079.639299	240058.258523	53.778855
3078.744830	239914.220220	53.783860
3078.183013	239772.319390	53.788865
3077.331869	239636.754236	53.793869
3077.036264	239499.064168	53.798874
3076.485854	239365.641676	53.803879
3075.861346	239225.177454	53.808884
3075.324818	239078.893626	53.813889
3074.129232	238939.640574	53.818893
3073.782218	238796.968507	53.823898
3072.948150	238653.788034	53.828903
3072.330807	238522.592523	53.833908
3071.870969	238376.934082	53.838913
3070.851704	238250.640692	53.843917
3070.367565	238099.740862	53.848922
3069.248071	237966.461048	53.853927
3069.036704	237840.575006	53.858932
3068.711702	237692.833552	53.863937
3067.802434	237562.551172	53.868941
3067.298900	237412.801244	53.873946
3066.543978	237270.959645	53.878951
3065.584823	237137.171665	53.883956
3064.912158	236982.483662	53.888961
3064.324860	236853.551695	53.893965
3063.736284	236715.886029	53.898970
3062.814575	236581.277985	53.903975
3062.165811	236436.237740	53.908980
3061.856448	236301.253036	53.913985
3060.871283	236176.790081	53.918989
3060.316078	236031.913835	53.923994
3059.534988	235893.999623	53.928999
3058.979770	235758.570731	53.934004
3058.192468	235615.641567	53.939009
3057.320668	235480.823345	53.944013
3056.817718	235348.467797	53.949018
3056.190922	235214.145880	53.954023
3055.393230	235080.080361	53.959028
3055.244821	234941.099689	53.964033
3054.255864	234809.280109	53.969037
3053.952371	234667.319697	53.974042
3053.163459	234533.788244	53.979047
3052.242166	234396.789471	53.984052
3051.836611	234262.561124	53.989057
3051.227551	234120.242447	53.994061
3050.615183	233982.940719	53.999066
3049.768057	233862.303686	54.004071
3048.872922	233718.986887	54.009076
3048.250882	233563.710416	54.014081
3047.430312	233439.275725	54.019085
3046.813177	233297.927111	54.024090
3046.311397	233169.521026	54.029095
3045.912095	233039.036404	54.034100
3045.168182	232898.930656	54.039105
3044.498572	232767.419752	54.044109
3044.015874	232627.069353	54.049114
3043.042630	232494.180976	54.054119
3042.290663	232361.283223	54.059124
3041.981021	232202.954913	54.064129
3040.911764	232079.961795	54.069133
3040.411447	231937.450891	54.074138
3039.815530	231803.561648	54.079143
3038.979502	231669.990690	54.084148
3038.399077	231532.101783	54.089153
3037.561040	231407.239660	54.094157
3036.894440	231275.628515	54.099162
3036.604760	231136.675682	54.104167
3035.525390	231000.827140	54.109172
3035.018349	230856.612988	54.114177
3033.932638	230734.158967	54.119181
3033.499871	230606.738488	54.124186
3032.976781	230473.043346	54.129191
3032.591778	230341.057964	54.134196
3032.044317	230192.191704	54.139201
3031.284945	230069.992469	54.144205
3030.488367	229922.566498	54.149210
3029.740273	229791.454176	54.154215
3028.855963	229662.095016	54.159220
3028.592346	229524.490007	54.164225
3028.073074	229392.578196	54.169229
3027.447724	229252.535612	54.174234
3025.883320	229118.523550	54.179239
3025.296381	228976.794850	54.184244
3024.890199	228843.669261	54.189249
3023.571379	228716.748198	54.194253
3023.515187	228583.134757	54.199258
3022.948030	228457.902859	54.204263
3022.099013	228331.009838	54.209268
3021.678761	228197.250926	54.214273
3021.015645	228073.053232	54.219277
3020.485284	227932.259350	54.224282
3019.726285	227797.052461	54.229287
3018.614354	227671.220484	54.234292
3018.403090	227532.795570	54.239297
3017.673289	227415.509384	54.244301
3017.102587	227274.977583	54.249306
3016.183603	227146.824335	54.254311
3015.537899	227028.303239	54.259316
3014.937511	226887.573093	54.264321
3014.205965	226762.293319	54.269325
3013.894363	226629.665418	54.274330
3013.227367	226503.879324	54.279335
3012.591683	226371.455899	54.284340
3012.021043	226227.730499	54.289345
3011.237500	226104.687770	54.294349
3010.801898	225949.687795	54.299354
3010.070788	225817.509509	54.304359
3009.248772	225690.641649	54.309364
3008.925025	225553.841838	54.314369
3008.208944	225422.132832	54.319373
3007.405429	225274.155850	54.324378
3006.801558	225141.907593	54.329383
3006.202537	225012.357594	54.334388
3005.732656	224864.137592	54.339393
3004.507838	224732.548430	54.344397
3004.189771	224587.792977	54.349402
3003.440053	224448.096334	54.354407
3002.353378	224320.623279	54.359412
3001.993022	224190.998633	54.364417
3001.329585	224044.860333	54.369421
3000.712601	223917.466333	54.374426
3000.261643	223777.010690	54.379431
2999.293546	223636.229801	54.384436
2998.730114	223498.631253	54.389441
2997.882807	223381.331278	54.394445
2997.217689	223248.446628	54.399450
2996.784494	223113.106803	54.404455
2995.707603	222978.429228	54.409460
2995.427633	222845.026019	54.414465
2994.711595	222714.632670	54.419469
2993.989013	222579.097718	54.424474
2993.268313	222445.739507	54.429479
2992.318182	222319.241022	54.434484
2991.710100	222190.982806	54.439489
2990.815415	222058.938518	54.444493
2990.350838	221923.491178	54.449498
2989.750934	221804.194053	54.454503
2989.066360	221678.265617	54.459508
2988.631275	221536.423989	54.464513
2987.650758	221418.995337	54.469517
2987.078865	221284.890010	54.474522
2986.480209	221158.706974	54.479527
2985.878408	221036.038016	54.484532
2985.308067	220888.299761	54.489537
2984.520341	220765.584301	54.494541
2983.903105	220634.313274	54.499546
2983.206395	220502.978682	54.504551
2982.175399	220379.895027	54.509556
2981.988887	220246.137897	54.514561
2981.068152	220124.806606	54.519565
2980.720638	219991.520955	54.524570
2979.808266	219872.594614	54.529575
2979.188373	219736.602998	54.534580
2978.913252	219600.315196	54.539585
2977.827324	219471.411720	54.544589
2977.150719	219342.927385	54.549594
2976.620869	219212.968906	54.554599
2975.798586	219084.342611	54.559604
2975.303276	218953.513540	54.564609
2974.321754	218833.377840	54.569613
2973.866008	218695.949243	54.574618
2973.242329	218563.231826	54.579623
2972.369808	218444.874331	54.584628
2972.159064	218308.960643	54.589633
2971.183476	218189.283331	54.594637
2970.700876	218059.306728	54.599642
2969.804117	217928.759478	54.604647
2969.030712	217805.206632	54.609652
2968.615384	217677.473116	54.614657
2967.776699	217555.585812	54.619661
2967.066443	217427.352095	54.624666
2966.572881	217297.696851	54.629671
2965.658248	217177.336970	54.634676
2965.459793	217042.276607	54.639681
2964.854797	216916.458378	54.644685
2964.018891	216787.889316	54.649690
2963.413342	216661.664312	54.654695
2962.784404	216531.981008	54.659700
2962.179981	216395.904223	54.664705
2961.449249	216281.804791	54.669709
2960.808502	216136.149522	54.674714
2960.463169	216006.562322	54.679719
2959.154377	215884.306871	54.684724
2959.024110	215748.219943	54.689729
2958.285772	215624.970909	54.694733
2957.135922	215490.929750	54.699738
2956.615807	215368.321248	54.704743
2956.215974	215232.239842	54.709748
2955.584180	215108.198435	54.714753
2954.873044	214977.016397	54.719757
2954.300900	214836.011680	54.724762
2953.594765	214717.341452	54.729767
2952.612266	214580.755371	54.734772
2952.222357	214445.972280	54.739777
2951.415722	214322.749165	54.744781
2950.740134	214196.718020	54.749786
2949.878040	214072.218585	54.754791
2949.454706	213934.768870	54.759796
2948.813369	213805.792805	54.764801
2947.646193	213686.217329	54.769805
2947.268934	213551.115844	54.774810
2946.682089	213432.441750	54.779815
2945.684517	213308.741624	54.784820
2945.810129	213177.710677	54.789825
2944.567744	213060.464773	54.794829
2943.803121	212925.107702	54.799834
2943.514937	212792.450201	54.804839
2942.723436	212673.988079	54.809844
2942.260856	212548.995524	54.814849
2941.813975	212414.645635	54.819853
2940.998009	212286.222063	54.824858
2940.091424	212162.115144	54.829863
2939.218472	212041.006933	54.834868
2939.027973	211900.253554	54.839873
2938.279516	211778.095167	54.844877
2937.450776	211653.378696	54.849882
2936.849511	211525.889968	54.854887
2936.026281	211392.212739	54.859892
2935.602355	211265.778317	54.864897
2934.796408	211141.682901	54.869901
2934.220161	211007.674638	54.874906
2933.692276	210882.568396	54.879911
2932.688956	210760.210491	54.884916
2932.240228	210628.091995	54.889921
2931.589916	210501.567668	54.894925
2930.895250	210367.604970	54.899930
2930.193418	210252.035044	54.904935
2929.352797	210135.367281	54.909940
2928.858354	210006.044669	54.914945
2928.055836	209876.822014	54.919949
2927.296007	209748.789251	54.924954
2926.960726	209622.955019	54.929959
2926.039767	209505.104778	54.934964
2925.559659	209377.919413	54.939969
2924.791808	209258.301748	54.944973
2924.238916	209125.362926	54.949978
2923.604426	208995.631869	54.954983
2922.921564	208869.574206	54.959988
2922.498637	208733.548376	54.964993
2921.485526	208610.483536	54.969997
2920.886367	208489.338847	54.975002
2920.013690	208354.225071	54.980007
2919.068480	208246.855568	54.985012
2918.540333	208119.744059	54.990017
2917.932339	207995.699966	54.995021
2917.100217	207872.557058	55.000026
2916.416720	207761.316126	55.005031
2915.643201	207654.136853	55.010036
2915.478929	207520.134570	55.015041
2914.421085	207407.859043	55.020045
2914.256371	207279.546332	55.025050
2913.586665	207153.706519	55.030055
2912.686567	207037.015918	55.035060
2911.862312	206912.041062	55.040065
2911.235117	206802.091141	55.045069
2911.035616	206675.694266	55.050074
2910.402882	206547.800860	55.055079
2909.652204	206431.787765	55.060084
2909.240080	206295.778468	55.065089
2908.212198	206179.580679	55.070093
2907.419863	206049.562808	55.075098
2906.816777	205919.426172	55.080103
2905.821252	205805.031189	55.085108
2905.558608	205680.250003	55.090113
2904.521390	205558.175228	55.095117
2904.328750	205428.929187	55.100122
2903.416939	205309.393116	55.105127
2902.898241	205194.414769	55.110132
2902.261791	205073.473846	55.115137
2901.541250	204952.011978	55.120141
2900.702062	204828.456566	55.125146
2900.316098	204708.049434	55.130151
2899.477753	204579.467491	55.135156
2899.012358	204457.126325	55.140161
2898.280861	204344.143224	55.145165
2897.625395	204212.542459	55.150170
2897.019396	204099.438159	55.155175
2896.043260	203971.464807	55.160180
2895.638664	203843.566684	55.165185
2894.913439	203724.246162	55.170189
2894.310389	203605.441044	55.175194
2893.741942	203488.768685	55.180199
2893.005715	203354.153873	55.185204
2892.342559	203236.758917	55.190209
2891.525137	203107.286159	55.195213
2891.096868	202983.300622	55.200218
2890.528670	202875.054119	55.205223
2889.676068	202740.586460	55.210228
2888.964193	202606.109565	55.215233
2888.198801	202501.305560	55.220237
2887.500801	202377.173186	55.225242
2886.741973	202256.168555	55.230247
2886.008404	202139.537872	55.235252
2885.565534	202020.150806	55.240257
2884.769600	201898.949215	55.245261
2884.290489	201779.924727	55.250266
2883.570643	201665.099924	55.255271
2882.745708	201539.576969	55.260276
2882.147051	201425.497017	55.265281
2881.458343	201299.253126	55.270285
2880.777851	201178.123918	55.275290
2880.423981	201053.087405	55.280295
2879.599031	200945.178014	55.285300
2879.067667	200820.081061	55.290305
2878.509225	200701.529588	55.295309
2878.019124	200575.370445	55.300314
2877.413278	200450.273409	55.305319
2876.289131	200327.969248	55.310324
2875.762766	200198.457215	55.315329
2874.743053	200087.233592	55.320333
2874.343413	199968.874902	55.325338
2873.829376	199845.151786	55.330343
2873.054125	199721.572120	55.335348
2872.493331	199603.494256	55.340353
2871.471874	199481.786564	55.345357
2870.940429	199359.378018	55.350362
2870.165472	199234.755962	55.355367
2869.425369	199120.028822	55.360372
2868.847620	199005.721598	55.365377
2868.476755	198882.041658	55.370381
2867.701589	198767.791656	55.375386
2867.138366	198639.638076	55.380391
2866.460017	198524.164391	55.385396
2866.028724	198405.534222	55.390401
2864.915215	198294.227385	55.395405
2864.170380	198154.116860	55.400410
2863.716501	198046.523557	55.405415
2863.032144	197929.525140	55.410420
2862.212119	197798.029461	55.415425
2861.824043	197694.193002	55.420429
2861.315527	197567.204043	55.425434
2860.419131	197444.234205	55.430439
2859.512408	197329.397371	55.435444
2859.385395	197198.035224	55.440449
2858.396623	197084.649809	55.445453
2857.781374	196957.653787	55.450458
2857.130785	196844.711601	55.455463
2856.522077	196740.415722	55.460468
2856.212515	196603.536083	55.465473
2855.210362	196484.758906	55.470477
2854.480817	196364.831804	55.475482
2853.575212	196241.471819	55.480487
2853.007034	196121.557903	55.485492
2852.813981	195994.357421	55.490497
2851.555404	195888.003040	55.495501
2851.066337	195765.468939	55.500506
2850.371758	195647.141240	55.505511
2849.943340	195525.501533	55.510516
2848.984237	195406.770934	55.515521
2848.411338	195297.179042	55.520525
2847.764582	195172.864501	55.525530
2847.356178	195057.902928	55.530535
2846.327450	194933.738533	55.535540
2845.925695	194813.724992	55.540545
2844.979002	194706.954695	55.545549
2844.663025	194581.100511	55.550554
2843.668703	194461.257995	55.555559
2843.155117	194342.701095	55.560564
2842.443276	194228.031220	55.565569
2841.736634	194109.250967	55.570573
2841.329758	193981.351409	55.575578
2840.286163	193863.490323	55.580583
2839.485772	193752.003797	55.585588
2839.152954	193632.885550	55.590593
2838.171721	193522.738725	55.595597
2838.015161	193413.632124	55.600602
2837.128472	193283.736377	55.605607
2836.456745	193172.905128	55.610612
2835.968846	193053.087583	55.615617
2835.102297	192938.457903	55.620621
2834.330034	192825.772986	55.625626
2833.638244	192703.367525	55.630631
2832.867148	192602.719398	55.635636
2832.331719	192471.574150	55.640641
2831.523034	192371.479558	55.645645
2831.179756	192255.712553	55.650650
2830.817924	192129.197498	55.655655
2830.002269	192013.353195	55.660660
2829.322809	191896.749645	55.665665
2828.566323	191784.662620	55.670669
2828.106771	191663.940622	55.675674
2827.404669	191547.812255	55.680679
2826.587271	191429.628543	55.685684
2826.130850	191308.563407	55.690689
2825.289304	191180.600010	55.695693
2824.942311	191071.745071	55.700698
2824.196532	190945.357519	55.705703
2823.224140	190827.008982	55.710708
2822.833164	190705.833207	55.715713
2822.061208	190594.056743	55.720717
2821.455541	190472.890111	55.725722
2820.671640	190347.260824	55.730727
2819.779579	190232.590676	55.735732
2819.346118	190115.010977	55.740737
2818.098465	190002.013504	55.745741
2817.827925	189895.808194	55.750746
2817.464653	189777.811080	55.755751
2816.632074	189657.662107	55.760756
2816.070685	189540.269483	55.765761
2815.163395	189423.657124	55.770765
2814.694923	189309.011176	55.775770
2813.973888	189191.606533	55.780775
2813.243146	189080.768568	55.785780
2812.770477	188953.694190	55.790785
2812.095545	188852.313498	55.795789
2811.139149	188728.675084	55.800794
2810.417236	188615.139651	55.805799
2809.559486	188509.386686	55.810804
2809.102318	188390.809955	55.815809
2808.391524	188288.647372	55.820813
2807.912531	188173.064405	55.825818
2807.445632	188051.067770	55.830823
2806.283611	187945.122549	55.835828
2806.110167	187817.813028	55.840833
2805.231393	187719.520413	55.845837
2804.782175	187598.323664	55.850842
2804.338134	187481.820881	55.855847
2803.401721	187370.612441	55.860852
2802.896050	187244.094994	55.865857
2801.997437	187129.522519	55.870861
2800.935649	187013.411365	55.875866
2800.886896	186898.348645	55.880871
2799.654456	186787.646488	55.885876
2799.000455	186677.221920	55.890881
2798.665813	186571.085201	55.895885
2798.538337	186451.227193	55.900890
2797.581437	186335.406468	55.905895
2796.520016	186224.436872	55.910900
2795.937673	186099.461339	55.915905
2795.014885	185995.276487	55.920909
2794.533116	185879.597935	55.925914
2794.017227	185767.996015	55.930919
2793.229666	185655.076184	55.935924
2792.890195	185534.350927	55.940929
2792.079606	185428.762950	55.945933
2791.427759	185317.018294	55.950938
2790.999959	185196.664131	55.955943
2790.187843	185085.263471	55.960948
2789.674117	184971.665901	55.965953
2788.624371	184861.906334	55.970957
2788.052161	184746.702975	55.975962
2787.567939	184631.651354	55.980967
2786.585292	184515.495890	55.985972
2785.786070	184390.241402	55.990977
2785.378012	184290.762163	55.995981
2784.356417	184181.012528	56.000986
2783.879916	184056.165825	56.005991
2783.326877	183957.689823	56.010996
2782.800445	183837.075067	56.016001
2781.781496	183727.733207	56.021005
2781.409430	183610.084073	56.026010
2780.990486	183504.565813	56.031015
2780.060546	183402.614295	56.036020
2779.450538	183277.701880	56.041025
2778.582330	183177.471155	56.046029
2778.689700	183064.606929	56.051034
2777.814820	182939.406681	56.056039
2776.957585	182828.832949	56.061044
2776.305529	182709.386042	56.066049
2775.003739	182596.987911	56.071053
2774.690177	182482.830727	56.076058
2774.259607	182369.277526	56.081063
2773.406267	182265.370246	56.086068
2772.820708	182147.949644	56.091073
2772.095962	182035.296189	56.096077
2771.503107	181912.649209	56.101082
2771.028165	181804.319939	56.106087
2770.203690	181696.809532	56.111092
2769.346535	181574.917717	56.116097
2768.715936	181472.516227	56.121101
2767.847962	181360.141618	56.126106
2767.573226	181244.200673	56.131111
2766.528594	181135.747064	56.136116
2765.932000	181025.073028	56.141121
2765.186124	180916.305522	56.146125
2764.693962	180809.673265	56.151130
2764.124659	180703.396937	56.156135
2763.595987	180592.573331	56.161140
2763.267612	180466.454113	56.166145
2762.113090	180364.176406	56.171149
2761.518222	180243.404343	56.176154
2761.159299	180125.991498	56.181159
2760.339489	180026.549031	56.186164
2759.713520	179912.193716	56.191169
2759.159139	179799.633601	56.196173
2758.616483	179687.478963	56.201178
2758.016124	179555.007404	56.206183
2757.100238	179449.565006	56.211188
2756.540144	179321.247186	56.216193
2756.067900	179225.211325	56.221197
2754.806322	179105.451204	56.226202
2754.312797	178982.784149	56.231207
2753.443919	178878.823934	56.236212
2752.925974	178749.941507	56.241217
2752.480738	178648.713072	56.246221
2751.879785	178531.597372	56.251226
2751.265296	178408.684038	56.256231
2750.218694	178302.171338	56.261236
2749.543188	178189.660139	56.266241
2748.740349	178078.403197	56.271245
2748.428810	177968.188033	56.276250
2747.994118	177851.009741	56.281255
2747.111215	177736.421202	56.286260
2746.488651	177628.914540	56.291265
2745.713157	177518.850372	56.296269
2745.402097	177400.407277	56.301274
2744.497431	177279.985323	56.306279
2743.526880	177172.331459	56.311284
2742.697829	177053.869653	56.316289
2742.365556	176945.657384	56.321293
2741.639496	176834.645992	56.326298
2741.038248	176722.444978	56.331303
2740.397207	176616.673656	56.336308
2740.018464	176500.584150	56.341313
2738.931519	176393.955552	56.346317
2738.396481	176275.411253	56.351322
2737.979355	176164.874203	56.356327
2736.970183	176049.420028	56.361332
2736.407847	175932.165644	56.366337
2735.697093	175826.203903	56.371341
2734.752386	175713.945585	56.376346
2733.886981	175599.296624	56.381351
2733.240379	175497.624482	56.386356
2732.883991	175381.521888	56.391361
2732.243992	175284.885795	56.396365
2731.725778	175167.830117	56.401370
2731.245725	175054.965833	56.406375
2730.398187	174952.741834	56.411380
2729.842354	174848.856644	56.416385
2729.385625	174732.606462	56.421389
2728.718395	174616.504426	56.426394
2728.129771	174501.560356	56.431399
2727.130117	174383.082453	56.436404
2726.758508	174266.273245	56.441409
2725.959706	174161.652501	56.446413
2725.254422	174043.739440	56.451418
2724.536837	173930.063814	56.456423
2724.238413	173825.135754	56.461428
2723.372458	173698.282899	56.466433
2722.614750	173592.181837	56.471437
2721.927441	173467.730558	56.476442
2721.447157	173355.278055	56.481447
2720.341005	173247.935876	56.486452
2720.143473	173132.323319	56.491457
2719.175012	173026.804018	56.496461
2719.056521	172905.418413	56.501466
2718.230577	172774.988456	56.506471
2717.015240	172674.049447	56.511476
2716.550965	172562.423304	56.516481
2715.979634	172450.178552	56.521485
2715.404573	172334.195727	56.526490
2714.732451	172229.381948	56.531495
2714.000624	172122.352332	56.536500
2713.568845	171997.203876	56.541505
2712.463662	171889.750774	56.546509
2711.865671	171770.962677	56.551514
2711.075633	171660.726027	56.556519
2710.432091	171556.481798	56.561524
2709.878041	171434.381241	56.566529
2709.307073	171333.534355	56.571533
2709.058774	171222.233885	56.576538
2708.140589	171106.423501	56.581543
2707.523279	170983.749381	56.586548
2706.910766	170871.973488	56.591553
2705.878682	170771.582620	56.596557
2705.402506	170650.502267	56.601562
2704.936404	170531.697046	56.606567
2703.832147	170426.714936	56.611572
2703.674293	170311.778394	56.616577
2702.916020	170192.944196	56.621581
2702.104490	170084.050695	56.626586
2701.801707	169965.157754	56.631591
2701.214730	169845.420026	56.636596
2700.089938	169734.656900	56.641601
2699.449558	169623.206948	56.646605
2698.984866	169508.563025	56.651610
2698.208446	169377.195549	56.656615
2697.669126	169272.940951	56.661620
2697.325509	169150.814256	56.666625
2696.431633	169045.268490	56.671629
2696.309655	168917.321395	56.676634
2695.041213	168796.982776	56.681639
2694.284735	168682.400270	56.686644
2693.710914	168556.560597	56.691649
2693.247225	168447.947264	56.696653
2692.178675	168328.468603	56.701658
2691.758186	168209.510746	56.706663
2690.899267	168098.646665	56.711668
2689.955352	167993.226192	56.716673
2689.524908	167871.206369	56.721677
2689.213494	167752.296247	56.726682
2688.477835	167638.158662	56.731687
2687.486222	167524.265428	56.736692
2687.258634	167399.824374	56.741697
2686.357972	167284.010058	56.746701
2685.689978	167174.440904	56.751706
2685.137665	167057.402233	56.756711
2684.674831	166940.031854	56.761716
2683.907241	166817.967129	56.766721
2682.893151	166700.621257	56.771725
2682.032592	166580.441255	56.776730
2681.995644	166470.201976	56.781735
2680.498396	166374.321468	56.786740
2680.313484	166253.488701	56.791745
2679.318923	166144.788102	56.796749
2678.760761	166031.021474	56.801754
2678.694693	165910.438017	56.806759
2677.800639	165803.489947	56.811764
2677.155003	165677.022805	56.816769
2676.382226	165572.281385	56.821773
2675.763165	165451.888754	56.826778
2675.349550	165331.374958	56.831783
2674.473705	165217.534005	56.836788
2673.845793	165098.046713	56.841793
2673.092490	164981.987341	56.846797
2672.296521	164874.861122	56.851802
2671.950542	164758.941361	56.856807
2670.945707	164650.259501	56.861812
2670.435090	164523.991077	56.866817
2669.885649	164418.988683	56.871821
2669.045909	164296.829265	56.876826
2668.704679	164178.113300	56.881831
2667.780711	164070.272249	56.886836
2667.425947	163940.141257	56.891841
2666.758567	163830.429328	56.896845
2665.821394	163718.204812	56.901850
2665.563916	163597.811834	56.906855
2664.763707	163479.031002	56.911860
2664.188784	163361.969481	56.916865
2663.196670	163235.362222	56.921869
2662.743231	163118.917966	56.926874
2662.083338	163001.031915	56.931879
2661.291251	162905.036047	56.936884
2660.548659	162768.486329	56.941889
2659.937085	162657.535809	56.946893
2659.343971	162538.025964	56.951898
2658.764618	162422.710049	56.956903
2658.149424	162308.493607	56.961908
2657.552659	162188.896500	56.966913
2656.380399	162079.295305	56.971917
2655.667608	161958.356935	56.976922
2655.638587	161833.636267	56.981927
2654.377474	161717.845789	56.986932
2654.063580	161599.095814	56.991937
2653.160573	161478.443484	56.996941
2652.706217	161369.709693	57.001946
2652.101732	161251.210340	57.006951
2651.167455	161138.522998	57.011956
2650.940739	161014.141646	57.016961
2649.948451	160906.740451	57.021965
2649.148920	160782.081972	57.026970
2648.746425	160667.404813	57.031975
2647.963705	160563.607561	57.036980
2647.328462	160449.184117	57.041985
2646.740072	160330.125892	57.046989
2646.210531	160208.910163	57.051994
2645.662784	160088.994507	57.056999
2644.802292	159971.620640	57.062004
2644.415094	159842.552157	57.067009
2643.801379	159731.216979	57.072013
2642.760792	159605.075252	57.077018
2642.031233	159487.135587	57.082023
2641.414330	159371.886378	57.087028
2640.998842	159254.406259	57.092033
2640.319961	159129.798076	57.097037
2639.419307	159021.383780	57.102042
2638.917694	158896.710202	57.107047
2637.947214	158780.196813	57.112052
2637.683840	158655.702469	57.117057
2637.225187	158551.694551	57.122061
2636.329684	158428.000390	57.127066
2635.942555	158290.737835	57.132071
2635.083012	158180.794108	57.137076
2634.336068	158059.226179	57.142081
2633.962261	157939.341188	57.147085
2632.964056	157817.330839	57.152090
2632.185731	157688.878941	57.157095
2631.580540	157582.875850	57.162100
2630.930414	157449.205103	57.167105
2629.973994	157342.152418	57.172109
2629.632418	157234.163625	57.177114
2629.117299	157104.985728	57.182119
2628.271166	156992.946123	57.187124
2628.147200	156870.050578	57.192129
2627.136377	156755.965742	57.197133
2626.386760	156632.890515	57.202138
2625.752097	156510.255153	57.207143
2625.024154	156384.393427	57.212148
2624.611742	156251.706647	57.217153
2623.467693	156144.267941	57.222157
2623.097365	156029.181491	57.227162
2622.620553	155902.086828	57.232167
2621.863832	155784.812422	57.237172
2621.052949	155658.241945	57.242177
2620.321129	155545.807624	57.247181
2620.013230	155418.128688	57.252186
2619.347610	155300.523727	57.257191
2618.175841	155190.728060	57.262196
2617.724002	155061.497033	57.267201
2616.933626	154950.205303	57.272205
2616.600808	154825.252827	57.277210
2615.917364	154717.160935	57.282215
2615.090656	154591.474053	57.287220
2614.549526	154465.513583	57.292225
2613.727360	154341.720910	57.297229
2613.130538	154223.180881	57.302234
2612.731964	154106.516542	57.307239
2611.817638	153981.583080	57.312244
2611.499878	153858.246135	57.317249
2610.855305	153739.486583	57.322253
2610.017021	153613.245916	57.327258
2609.560311	153488.318050	57.332263
2608.548193	153368.918954	57.337268
2608.221570	153241.505474	57.342273
2607.304446	153128.371380	57.347277
2606.696002	152989.322237	57.352282
2606.126958	152863.791687	57.357287
2605.049831	152753.455174	57.362292
2604.502282	152631.036227	57.367297
2604.216340	152503.949609	57.372301
2603.469993	152383.024804	57.377306
2602.743685	152256.771553	57.382311
2601.973563	152131.212094	57.387316
2601.861077	152004.125332	57.392321
2600.980154	151878.762339	57.397325
2600.466537	151750.011511	57.402330
2599.682684	151639.022157	57.407335
2598.874949	151509.162243	57.412340
2598.447304	151366.545129	57.417345
2597.352715	151254.614923	57.422349
2596.669834	151128.943791	57.427354
2596.180692	151007.563857	57.432359
2595.554845	150889.968200	57.437364
2594.736531	150756.782928	57.442369
2594.174666	150642.991008	57.447373
2593.491982	150520.804702	57.452378
2593.326083	150370.804158	57.457383
2592.330346	150199.888477	57.462388
2591.973095	150083.295368	57.467393
2591.017585	149957.811766	57.472397
2590.493714	149819.639625	57.477402
2590.039004	149716.204999	57.482407
2589.086056	149558.707205	57.487412
2588.389916	149445.067862	57.492417
2587.601945	149297.267925	57.497421
2586.698407	149190.690635	57.502426
2586.413598	149061.965023	57.507431
2585.617422	148927.868699	57.512436
2585.116930	148812.497548	57.517441
2584.271141	148681.638250	57.522445
2583.336707	148559.346751	57.527450
2583.173294	148459.415838	57.532455
2582.315325	148312.622832	57.537460
2581.643056	148182.894593	57.542465
2580.758664	148067.396331	57.547469
2580.152264	147907.322655	57.552474
2579.716080	147817.171944	57.557479
2579.263560	147689.838267	57.562484
2578.498894	147549.362945	57.567489
2577.770739	147436.155196	57.572493
2577.117372	147309.109046	57.577498
2576.334710	147160.263337	57.582503
2575.280743	147067.785326	57.587508
2574.977801	146909.028400	57.592513
2574.176768	146811.186224	57.597517
2573.738197	146658.374162	57.602522
2573.233769	146582.826944	57.607527
2571.914380	146446.511084	57.612532
2571.057183	146312.435460	57.617537
2571.245324	146174.077310	57.622541
2570.430430	146094.145327	57.627546
2569.954649	145973.964202	57.632551
2568.747553	145825.827460	57.637556
2568.930469	145669.109312	57.642561
2567.785056	145578.912185	57.647565
2566.845113	145433.886518	57.652570
2566.919207	145305.678416	57.657575
2565.882490	145199.072124	57.662580
2565.310495	145042.667367	57.667585
2564.438232	144949.633084	57.672589
2564.169613	144798.976156	57.677594
2563.520356	144667.695711	57.682599
2562.486300	144557.101035	57.687604
2562.292456	144410.754680	57.692609
2561.184808	144294.708414	57.697613
2560.999582	144149.696200	57.702618
2560.520545	144008.238429	57.707623
2559.247066	143910.785189	57.712628
2558.652139	143754.149124	57.717633
2558.136603	143627.350230	57.722637
2557.329593	143501.830634	57.727642
2556.829940	143370.366794	57.732647
2555.667527	143231.663943	57.737652
2555.652480	143109.667326	57.742657
2554.695692	142975.926848	57.747661
2553.914435	142867.089835	57.752666
2553.507142	142710.797843	57.757671
2552.608882	142595.360140	57.762676
2552.132209	142464.137969	57.767681
2551.226389	142342.031448	57.772685
2550.764393	142214.848710	57.777690
2550.227486	142095.467436	57.782695
2549.707712	141960.137369	57.787700
2549.139414	141817.649214	57.792705
2548.309608	141688.608308	57.797709
2547.441421	141550.806730	57.802714
2547.134203	141434.314083	57.807719
2546.325553	141303.886487	57.812724
2545.505360	141140.298438	57.817729
2544.980610	141038.809535	57.822733
2544.411370	140881.523418	57.827738
2543.498490	140760.822035	57.832743
2542.945392	140617.866998	57.837748
2542.287179	140503.466502	57.842753
2541.353305	140363.940054	57.847757
2540.719298	140241.646456	57.852762
2540.376636	140122.597940	57.857767
2539.574731	139976.394625	57.862772
2539.027973	139860.136607	57.867777
2538.186760	139720.344356	57.872781
2537.448064	139594.093182	57.877786
2537.019280	139459.204602	57.882791
2536.403729	139334.624818	57.887796
2535.927487	139189.097940	57.892801
2535.157376	139078.570309	57.897805
2534.464383	138930.004393	57.902810
2533.984026	138786.347788	57.907815
2533.143860	138666.913835	57.912820
2532.591704	138536.368693	57.917825
2531.590410	138395.921961	57.922829
2531.125313	138230.413208	57.927834
2530.401348	138123.185078	57.932839
2529.670370	138007.827418	57.937844
2528.946721	137840.722913	57.942849
2528.283930	137734.629918	57.947853
2527.869421	137613.188949	57.952858
2527.210974	137447.994725	57.957863
2526.540318	137348.205797	57.962868
2526.289458	137173.305838	57.967873
2525.308078	137083.438358	57.972877
2524.361912	136927.096770	57.977882
2524.317756	136770.447896	57.982887
2523.270026	136657.318155	57.987892
2522.568959	136536.104917	57.992897
2521.579002	136391.117894	57.997901
2520.962342	136228.324981	58.002906
2520.768246	136141.282937	58.007911
2519.621628	135997.313608	58.012916
2519.101034	135844.060923	58.017921
2518.907292	135713.966963	58.022925
2517.736832	135605.523033	58.027930
2517.588335	135441.898093	58.032935
2516.227806	135321.937761	58.037940
2516.031377	135179.041429	58.042945
2515.355577	135052.126497	58.047949
2515.218604	134904.813998	58.052954
2514.195651	134773.648865	58.057959
2513.659151	134645.786296	58.062964
2512.790637	134496.991214	58.067969
2512.262212	134349.400607	58.072973
2511.403334	134234.167075	58.077978
2511.120703	134085.586131	58.082983
2509.928523	133937.010388	58.087988
2509.272119	133807.023753	58.092993
2508.625314	133658.121657	58.097997
2508.241596	133517.028948	58.103002
2507.364263	133409.169268	58.108007
2506.517686	133261.596578	58.113012
2505.993735	133108.524102	58.118017
2505.062555	133006.619292	58.123021
2504.896095	132847.114878	58.128026
2504.203693	132711.067153	58.133031
2503.285491	132590.146270	58.138036
2503.102329	132438.446043	58.143041
2502.321058	132312.017250	58.148045
2501.604522	132181.298126	58.153050
2500.899346	132043.375704	58.158055
2500.309624	131887.462253	58.163060
2499.354328	131753.391504	58.168065
2498.742016	131628.590242	58.173069
2497.849927	131498.803937	58.178074
2497.832583	131365.348473	58.183079
2497.157387	131222.052445	58.188084
2496.306658	131065.880063	58.193089
2495.655386	130938.865239	58.198093
2494.935938	130801.992684	58.203098
2494.401289	130665.840893	58.208103
2493.606378	130528.283054	58.213108
2493.044497	130372.132256	58.218113
2492.408536	130256.333403	58.223117
2492.175484	130102.113394	58.228122
2491.188372	129953.830898	58.233127
2490.240332	129835.136587	58.238132
2490.018515	129677.030604	58.243137
2489.296516	129557.831707	58.248141
2488.509658	129396.247904	58.253146
2487.559130	129278.229514	58.258151
2487.281279	129108.133331	58.263156
2486.692646	128982.565371	58.268161
2485.799567	128828.787258	58.273165
2485.128643	128701.633332	58.278170
2484.854523	128557.779388	58.283175
2484.171213	128410.015808	58.288180
2483.307962	128258.585726	58.293185
2482.456663	128120.312124	58.298189
2482.083060	127987.170606	58.303194
2481.451767	127834.385259	58.308199
2480.420031	127700.092134	58.313204
2479.976772	127551.228300	58.318209
2479.060641	127411.203232	58.323213
2478.059514	127267.445871	58.328218
2477.614393	127107.040501	58.333223
2476.534215	127008.064095	58.338228
2476.244659	126877.632399	58.343233
2475.556696	126729.497609	58.348237
2474.864665	126608.160480	58.353242
2474.276222	126451.147083	58.358247
2473.566550	126310.294861	58.363252
2473.386650	126187.506879	58.368257
2472.687074	126045.117798	58.373261
2471.702156	125901.263478	58.378266
2471.047230	125760.621315	58.383271
2470.416693	125625.538254	58.388276
2469.627330	125496.703608	58.393281
2469.260823	125347.255485	58.398285
2468.877785	125205.353999	58.403290
2467.659647	125077.376659	58.408295
2467.085339	124936.510121	58.413300
2466.836011	124786.424282	58.418305
2465.810148	124659.053389	58.423309
2465.371121	124506.370548	58.428314
2464.344426	124367.153334	58.433319
2463.775392	124245.197775	58.438324
2463.299981	124092.027814	58.443329
2462.688783	123972.086535	58.448333
2462.488380	123796.017569	58.453338
2461.725388	123667.936702	58.458343
2460.745246	123527.611726	58.463348
2460.390063	123372.306228	58.468353
2459.659971	123244.399953	58.473357
2458.559423	123099.029798	58.478362
2458.144964	122952.294583	58.483367
2457.480656	122798.488995	58.488372
2456.482953	122659.199905	58.493377
2455.960776	122529.435629	58.498381
2455.171804	122400.158700	58.503386
2454.823157	122234.980039	58.508391
2454.016076	122109.402392	58.513396
2453.384231	121973.322170	58.518401
2452.601225	121812.532133	58.523405
2451.851467	121698.248011	58.528410
2451.429201	121540.259342	58.533415
2450.868507	121406.392780	58.538420
2450.300424	121261.227649	58.543425
2449.591731	121119.120199	58.548429
2448.937304	120966.669590	58.553434
2448.314981	120822.455056	58.558439
2446.809091	120705.184381	58.563444
2446.606170	120534.241614	58.568449
2446.014072	120429.244736	58.573453
2445.340368	120265.412328	58.578458
2444.683093	120131.688199	58.583463
2444.514742	120000.242446	58.588468
2443.641689	119847.242629	58.593473
2442.646544	119702.382377	58.598477
2442.152962	119554.389964	58.603482
2441.644084	119412.704483	58.608487
2440.792293	119278.767994	58.613492
2440.489572	119131.572980	58.618497
2439.809857	118980.648812	58.623501
2439.127230	118832.893616	58.628506
2438.448536	118682.935910	58.633511
2437.544154	118542.479553	58.638516
2436.899336	118408.698841	58.643521
2436.101264	118250.288186	58.648525
2435.363899	118116.764876	58.653530
2435.237172	117967.898158	58.658535
2434.379296	117830.129753	58.663540
2433.888238	117685.245314	58.668545
2433.149864	117538.274441	58.673549
2432.580481	117400.843460	58.678554
2431.808270	117252.038784	58.683559
2430.979670	117103.694586	58.688564
2430.497225	116950.783300	58.693569
2429.619115	116809.983133	58.698573
2429.160733	116671.237241	58.703578
2428.343163	116518.083344	58.708583
2427.559940	116375.385357	58.713588
2427.346030	116239.910023	58.718593
2426.623626	116100.675917	58.723597
2426.010841	115944.700196	58.728602
2425.358575	115793.561916	58.733607
2424.807715	115650.621699	58.738612
2423.907463	115500.946243	58.743617
2423.358534	115350.092537	58.748621
2422.413375	115203.491607	58.753626
2422.077611	115047.090318	58.758631
2421.112158	114901.262348	58.763636
2420.515078	114755.903615	58.768641
2419.993168	114617.248836	58.773645
2419.048521	114461.791844	58.778650
2418.587042	114313.437482	58.783655
2418.030522	114169.751265	58.788660
2417.214325	114029.635841	58.793665
2416.723116	113886.975411	58.798669
2415.860333	113733.109323	58.803674
2415.048806	113599.063001	58.808679
2414.863734	113442.432005	58.813684
2413.924137	113284.385740	58.818689
2413.099173	113163.221090	58.823693
2412.478563	113010.469778	58.828698
2412.001114	112850.119022	58.833703
2411.002822	112726.058256	58.838708
2410.816852	112555.807170	58.843713
2410.080344	112433.730856	58.848717
2409.169129	112287.097175	58.853722
2408.862399	112103.642596	58.858727
2407.864118	111991.478420	58.863732
2407.801889	111824.931623	58.868737
2406.919774	111674.844613	58.873741
2406.038683	111521.966055	58.878746
2405.389843	111380.810924	58.883751
2404.635475	111238.366044	58.888756
2404.062971	111089.020416	58.893761
2403.533016	110948.305823	58.898765
2402.616822	110795.551560	58.903770
2401.666853	110641.502691	58.908775
2400.641066	110511.130535	58.913780
2400.220300	110364.309939	58.918785
2399.529854	110227.521256	58.923789
2398.996709	110074.805931	58.928794
2398.308254	109951.255721	58.933799
2398.025707	109809.930963	58.938804
2397.560205	109646.572217	58.943809
2396.722621	109514.094158	58.948813
2396.238682	109376.179702	58.953818
2395.367319	109228.054028	58.958823
2394.926755	109078.154014	58.963828
2393.992965	108922.178031	58.968833
2393.214738	108792.886247	58.973837
2392.516746	108618.244679	58.978842
2392.045612	108504.686692	58.983847
2390.775285	108354.529288	58.988852
2390.716938	108208.996712	58.993857
2390.190995	108076.045599	58.998861
2389.675806	107894.946190	59.003866
2388.962972	107768.441384	59.008871
2388.402811	107640.498072	59.013876
2387.960715	107456.109936	59.018881
2387.284064	107326.644905	59.023885
2386.219882	107168.435719	59.028890
2385.991274	107013.527710	59.033895
2384.921274	106879.768468	59.038900
2384.920848	106690.214851	59.043905
2383.860440	106576.917988	59.048909
2382.984368	106429.825381	59.053914
2382.478059	106232.202525	59.058919
2381.763892	106127.773607	59.063924
2381.335852	105952.740553	59.068929
2380.376574	105811.191154	59.073933
2379.436286	105651.500383	59.078938
2379.276051	105512.953945	59.083943
2378.548896	105363.896509	59.088948
2377.875408	105191.623409	59.093953
2377.068155	105065.877452	59.098957
2376.460818	104888.330176	59.103962
2375.757086	104746.911543	59.108967
2375.073819	104608.218562	59.113972
2374.921467	104432.131538	59.118977
2373.927257	104282.380956	59.123981
2373.252921	104147.039013	59.128986
2372.955891	103976.554862	59.133991
2371.693544	103831.487226	59.138996
2371.491860	103670.195471	59.144001
2370.374628	103505.770129	59.149005
2369.723955	103383.326212	59.154010
2369.227246	103225.598848	59.159015
2368.201757	103073.348704	59.164020
2367.644684	102909.035377	59.169025
2367.220548	102765.027713	59.174029
2366.438635	102611.619086	59.179034
2366.215053	102476.031312	59.184039
2365.199659	102329.138519	59.189044
2364.374595	102170.556822	59.194049
2364.206023	102013.458009	59.199053
2363.162751	101863.863839	59.204058
2362.477868	101713.998121	59.209063
2361.530815	101561.034909	59.214068
2361.277898	101408.083162	59.219073
2360.300386	101256.319351	59.224077
2359.853742	101123.978225	59.229082
2359.143072	100950.137229	59.234087
2358.366667	100824.066563	59.239092
2357.840957	100646.037318	59.244097
2357.176917	100521.472860	59.249101
2356.619409	100344.167761	59.254106
2355.821056	100230.143133	59.259111
2355.508995	100056.290044	59.264116
2354.611882	99925.796914	59.269121
2354.252308	99744.627488	59.274125
2353.232258	99616.813318	59.279130
2352.951157	99447.273125	59.284135
2351.912805	99300.371450	59.289140
2351.606705	99156.849504	59.294145
2351.184516	98990.633323	59.299149
2350.084589	98827.766957	59.304154
2349.583006	98686.308630	59.309159
2348.973457	98531.713611	59.314164
2348.224752	98358.158251	59.319169
2347.190853	98223.307404	59.324173
2346.450405	98062.863089	59.329178
2346.106603	97914.046212	59.334183
2345.168966	97769.504146	59.339188
2344.879495	97583.958049	59.344193
2343.959194	97483.729433	59.349197
2343.392686	97291.443316	59.354202
2342.763630	97164.582946	59.359207
2342.297218	96995.489883	59.364212
2341.129342	96852.030290	59.369217
2341.191170	96688.734964	59.374221
2339.924852	96562.067810	59.379226
2339.866936	96392.248550	59.384231
2338.751273	96224.665793	59.389236
2338.193530	96099.068490	59.394241
2337.663530	95907.714262	59.399245
2337.129070	95789.934589	59.404250
2336.243590	95604.568979	59.409255
2335.654087	95470.291892	59.414260
2335.297865	95291.021859	59.419265
2334.489540	95138.009866	59.424269
2333.882437	94997.320584	59.429274
2333.241628	94829.032416	59.434279
2332.301918	94681.548906	59.439284
2331.995315	94518.904814	59.444289
2331.131704	94351.042405	59.449293
2330.326924	94205.817231	59.454298
2329.576214	94059.221026	59.459303
2329.159523	93875.450492	59.464308
2328.603031	93741.165860	59.469313
2327.746747	93593.460706	59.474317
2327.122757	93414.730113	59.479322
2326.521921	93245.876835	59.484327
2325.715570	93086.848134	59.489332
2324.861945	92957.624850	59.494337
2323.919239	92794.181108	59.499341
2323.556923	92629.207127	59.504346
2322.942908	92467.241855	59.509351
2322.314676	92339.933107	59.514356
2322.041410	92171.156552	59.519361
2321.237790	92034.886027	59.524365
2320.606409	91852.428127	59.529370
2319.808571	91702.418282	59.534375
2319.130623	91556.816250	59.539380
2318.281398	91392.905192	59.544385
2317.901009	91222.257040	59.549389
2316.962951	91098.060772	59.554394
2316.902189	90924.485634	59.559399
2315.491444	90767.319491	59.564404
2315.273962	90616.438814	59.569409
2314.390201	90473.685416	59.574413
2313.442682	90303.933241	59.579418
2313.143675	90167.955685	59.584423
2312.811150	89996.612061	59.589428
2311.726875	89844.301796	59.594433
2311.492873	89687.876140	59.599437
2310.403114	89518.298462	59.604442
2309.932143	89362.584774	59.609447
2308.983738	89209.838962	59.614452
2308.603346	89055.482553	59.619457
2307.877814	88905.296586	59.624461
2306.957997	88750.463641	59.629466
2306.313986	88573.538140	59.634471
2305.788593	88446.622485	59.639476
2305.449408	88279.167073	59.644481
2304.574269	88132.205426	59.649485
2303.941193	87969.946853	59.654490
2303.161501	87810.102782	59.659495
2302.226023	87654.088336	59.664500
2301.751390	87498.984560	59.669505
2301.132595	87349.445456	59.674509
2300.422984	87197.683980	59.679514
2300.123600	87036.121238	59.684519
2299.414402	86872.507370	59.689524
2298.727866	86708.897496	59.694529
2297.854283	86570.269753	59.699533
2297.251488	86411.504726	59.704538
2296.483262	86259.328126	59.709543
2295.590097	86111.070971	59.714548
2295.176538	85933.388976	59.719553
2294.428261	85797.199589	59.724557
2293.490767	85648.718135	59.729562
2293.427175	85488.219993	59.734567
2292.371924	85338.402852	59.739572
2291.595692	85183.427085	59.744577
2290.856756	85034.994493	59.749581
2290.423588	84884.555776	59.754586
2290.237747	84718.289231	59.759591
2289.401563	84565.539687	59.764596
2288.911697	84413.008880	59.769601
2288.386564	84260.237562	59.774605
2287.383304	84105.369071	59.779610
2286.847659	83934.207454	59.784615
2286.306368	83780.966781	59.789620
2285.491460	83620.367415	59.794625
2284.808125	83477.007626	59.799629
2284.127558	83311.984179	59.804634
2283.442988	83152.407188	59.809639
2282.779282	82999.299369	59.814644
2282.088686	82839.503875	59.819649
2281.324983	82683.131076	59.824653
2280.556091	82531.507448	59.829658
2279.844423	82374.951232	59.834663
2279.357722	82222.061860	59.839668
2278.549175	82050.654648	59.844673
2277.934879	81908.232640	59.849677
2277.264301	81749.982384	59.854682
2276.994507	81603.616413	59.859687
2275.992596	81448.729298	59.864692
2275.580142	81301.329680	59.869697
2275.034138	81135.345073	59.874701
2274.158166	80978.147274	59.879706
2273.268564	80816.022247	59.884711
2272.783792	80663.378492	59.889716
2272.213711	80509.557956	59.894721
2271.510016	80352.236178	59.899725
2270.936907	80192.404319	59.904730
2270.689959	80028.301345	59.909735
2269.602501	79878.300207	59.914740
2269.050732	79723.595399	59.919745
2268.407722	79564.850462	59.924750
2267.635688	79395.658364	59.929754
2267.138598	79223.648435	59.934759
2266.242749	79085.428548	59.939764
2265.506951	78920.017788	59.944769
2264.747700	78778.292993	59.949774
2263.886517	78617.530480	59.954778
2263.984249	78452.922793	59.959783
2263.031655	78295.877980	59.964788
2262.442387	78141.254389	59.969793
2262.071384	77987.921704	59.974798
2261.130837	77831.993789	59.979802
2260.246358	77650.407868	59.984807
2259.496494	77506.371218	59.989812
2259.222624	77341.299143	59.994817
2258.674766	77178.255148	59.999822
2257.726295	77011.911406	60.004826
2256.940595	76852.931314	60.009831
2256.265619	76706.537680	60.014836
2255.723349	76543.162069	60.019841
2255.335506	76382.310405	60.024846
2254.308954	76211.385566	60.029850
2254.011678	76052.473668	60.034855
2253.100546	75908.239488	60.039860
2252.647763	75739.717669	60.044865
2251.811992	75587.395506	60.049870
2251.200678	75416.975413	60.054874
2250.656527	75259.610493	60.059879
2249.670038	75092.319170	60.064884
2249.048181	74944.130513	60.069889
2248.372350	74790.369808	60.074894
2247.903015	74634.480444	60.079898
2247.197854	74474.004749	60.084903
2246.220520	74309.734200	60.089908
2245.808191	74150.475406	60.094913
2245.073350	73986.321093	60.099918
2244.735735	73840.528280	60.104922
2244.093350	73666.706865	60.109927
2243.098992	73513.297893	60.114932
2242.717421	73356.745677	60.119937
2241.941941	73199.915069	60.124942
2241.250075	73030.585978	60.129946
2240.885728	72865.419170	60.134951
2239.844762	72712.790286	60.139956
2239.144163	72556.713060	60.144961
2238.736861	72393.001348	60.149966
2237.853841	72233.813491	60.154970
2237.338724	72074.365841	60.159975
2236.672965	71915.437476	60.164980
2236.038715	71739.971883	60.169985
2235.531816	71590.548274	60.174990
2234.498743	71422.915003	60.179994
2234.144794	71263.245609	60.184999
2233.228532	71120.788774	60.190004
2232.621522	70923.421503	60.195009
2232.145170	70785.762136	60.200014
2231.019162	70616.117126	60.205018
2230.644880	70449.217423	60.210023
2230.045268	70309.915023	60.215028
2229.547878	70141.137195	60.220033
2228.411693	69988.823143	60.225038
2227.892937	69817.492504	60.230042
2227.211554	69651.756743	60.235047
2226.242301	69512.315946	60.240052
2225.923159	69356.102171	60.245057
2225.645750	69193.428823	60.250062
2224.912434	69027.795254	60.255066
2224.346517	68868.058589	60.260071
2223.584708	68715.042688	60.265076
2223.115147	68538.458470	60.270081
2222.355161	68379.573626	60.275086
2221.311135	68217.492363	60.280090
2220.864379	68051.910294	60.285095
2219.966841	67879.377366	60.290100
2219.479761	67729.986348	60.295105
2218.768999	67581.398293	60.300110
2217.679085	67402.807454	60.305114
2217.417258	67256.487653	60.310119
2216.703533	67098.061944	60.315124
2216.407224	66932.877211	60.320129
2215.296478	66770.289808	60.325134
2214.589350	66608.751192	60.330138
2214.433976	66440.261477	60.335143
2213.357261	66295.382798	60.340148
2212.853527	66125.735170	60.345153
2212.138440	65966.923152	60.350158
2211.511968	65813.582550	60.355162
2211.006957	65644.012194	60.360167
2209.987636	65489.571276	60.365172
2209.423619	65320.215782	60.370177
2208.841923	65162.681097	60.375182
2207.988369	65002.873141	60.380186
2207.509542	64843.557997	60.385191
2206.928034	64691.368563	60.390196
2206.784838	64518.799868	60.395201
2205.824336	64363.871106	60.400206
2205.061376	64202.190613	60.405210
2204.769597	64028.329648	60.410215
2204.077781	63858.041711	60.415220
2203.313479	63697.166723	60.420225
2202.834339	63529.627756	60.425230
2202.085436	63367.265094	60.430234
2201.642231	63180.217965	60.435239
2200.650018	63009.158968	60.440244
2199.575793	62857.587880	60.445249
2199.266795	62679.281240	60.450254
2198.470091	62517.652079	60.455258
2197.854251	62353.937836	60.460263
2197.237627	62192.039122	60.465268
2196.504907	62026.421464	60.470273
2195.646392	61856.811082	60.475278
2194.920510	61697.688113	60.480282
2194.663269	61524.563221	60.485287
2193.698042	61373.208346	60.490292
2193.391765	61203.285147	60.495297
2192.285530	61031.711328	60.500302
2191.684346	60874.535028	60.505306
2191.087082	60708.929624	60.510311
2190.487684	60550.929547	60.515316
2190.138398	60393.172851	60.520321
2189.277224	60214.571934	60.525326
2188.259967	60052.312025	60.530330
2188.020702	59889.401483	60.535335
2186.810766	59744.062166	60.540340
2186.560850	59564.240455	60.545345
2185.785147	59406.480591	60.550350
2185.008012	59234.060722	60.555354
2184.538750	59077.881976	60.560359
2183.631871	58911.221112	60.565364
2183.374743	58740.470519	60.570369
2182.447180	58589.572154	60.575374
2181.892491	58420.033326	60.580378
2181.471962	58251.155260	60.585383
2180.351469	58087.643810	60.590388
2179.808100	57937.139243	60.595393
2179.056037	57772.945440	60.600398
2178.631259	57602.415485	60.605402
2177.480176	57429.169677	60.610407
2176.946747	57299.174567	60.615412
2176.383521	57116.422719	60.620417
2175.681286	56955.342553	60.625422
2174.767163	56813.485966	60.630426
2174.126755	56652.284705	60.635431
2173.498250	56486.149032	60.640436
2172.717323	56323.349399	60.645441
2172.333767	56178.954499	60.650446
2171.798942	56016.814783	60.655450
2171.463979	55846.815330	60.660455
2170.572676	55687.273166	60.665460
2169.909902	55541.291445	60.670465
2169.376438	55364.637896	60.675470
2168.738826	55190.518417	60.680474
2167.937587	55038.594269	60.685479
2167.161587	54875.249754	60.690484
2166.558349	54710.803361	60.695489
2165.947232	54559.546062	60.700494
2165.302891	54395.029925	60.705498
2164.719480	54209.288200	60.710503
2163.716905	54090.595459	60.715508
2163.692051	53894.743533	60.720513
2162.569867	53744.039250	60.725518
2162.107592	53583.042460	60.730522
2161.182314	53410.245025	60.735527
2160.564966	53248.522708	60.740532
2160.121199	53073.838974	60.745537
2159.247965	52934.445645	60.750542
2158.806133	52759.334308	60.755546
2158.272654	52586.533201	60.760551
2157.485968	52446.345200	60.765556
2156.763608	52251.099470	60.770561
2156.006492	52114.133549	60.775566
2155.649419	51922.228448	60.780570
2154.903522	51786.981294	60.785575
2154.269237	51600.473911	60.790580
2153.709673	51449.152146	60.795585
2152.890661	51257.609010	60.800590
2152.121976	51117.637317	60.805594
2151.673038	50940.871089	60.810599
2150.876496	50772.666077	60.815604
2150.623909	50604.537696	60.820609
2149.586987	50435.823487	60.825614
2148.752982	50283.878053	60.830618
2148.408488	50107.249013	60.835623
2147.554388	49945.862851	60.840628
2147.045923	49783.259094	60.845633
2146.239747	49615.987113	60.850638
2145.403819	49442.055765	60.855642
2145.059121	49271.989957	60.860647
2144.307763	49109.589060	60.865652
2143.626360	48957.788894	60.870657
2143.323165	48771.606469	60.875662
2142.443651	48613.874393	60.880666
2141.815465	48438.815865	60.885671
2140.949894	48270.575825	60.890676
2140.231821	48123.245803	60.895681
2139.598536	47956.556727	60.900686
2139.005721	47774.688540	60.905690
2138.311604	47600.433256	60.910695
2137.745741	47443.199602	60.915700
2137.032094	47284.833068	60.920705
2136.288341	47115.357379	60.925710
2135.369880	46964.978405	60.930714
2134.962026	46770.966927	60.935719
2134.301011	46618.911577	60.940724
2133.753290	46457.910293	60.945729
2132.916124	46294.106532	60.950734
2131.991026	46124.526827	60.955738
2131.863484	45948.423566	60.960743
2131.102199	45789.360070	60.965748
2130.384091	45635.949587	60.970753
2129.953671	45459.953059	60.975758
2129.217211	45304.438764	60.980762
2128.516785	45126.125797	60.985767
2127.853316	44960.396620	60.990772
2127.439488	44795.432744	60.995777
2126.465686	44629.901432	61.000782
2125.668740	44462.591506	61.005786
2125.049529	44291.542033	61.010791
2124.022584	44146.097118	61.015796
2123.470060	43966.899660	61.020801
2123.045776	43800.975948	61.025806
2122.266351	43631.466933	61.030810
2121.758805	43474.519008	61.035815
2120.799467	43317.068618	61.040820
2120.422708	43142.734642	61.045825
2119.646340	42977.972037	61.050830
2119.071461	42823.956435	61.055834
2118.823432	42656.542042	61.060839
2118.277067	42487.380407	61.065844
2117.437404	42313.827109	61.070849
2116.707555	42142.816402	61.075854
2115.767238	41984.660467	61.080858
2115.261789	41817.728282	61.085863
2114.272574	41648.287820	61.090868
2113.732749	41478.600644	61.095873
2113.110711	41320.669094	61.100878
2112.379384	41158.174485	61.105882
2111.944054	40992.855006	61.110887
2110.929364	40833.387086	61.115892
2110.847742	40663.189421	61.120897
2110.073727	40487.487676	61.125902
2109.020217	40327.029874	61.130906
2108.528816	40158.185992	61.135911
2107.662659	39994.972866	61.140916
2107.382353	39828.523897	61.145921
2106.799563	39659.173004	61.150926
2106.182224	39497.923411	61.155930
2105.660675	39334.268286	61.160935
2104.733939	39165.025888	61.165940
2103.929524	38989.956181	61.170945
2103.483594	38828.288943	61.175950
2102.707990	38653.829906	61.180954
2102.223361	38502.194236	61.185959
2101.440965	38326.822779	61.190964
2100.777931	38151.966913	61.195969
2100.334612	37982.626402	61.200974
2099.588067	37810.914023	61.205978
2098.923688	37637.491084	61.210983
2097.924422	37481.009655	61.215988
2097.295871	37304.419892	61.220993
2096.900923	37134.729289	61.225998
2096.249054	36957.957172	61.231002
2095.490699	36796.082310	61.236007
2094.917027	36627.975770	61.241012
2094.144376	36452.875126	61.246017
2093.761051	36279.927347	61.251022
2092.929474	36113.731964	61.256026
2092.461351	35946.506932	61.261031
2091.499348	35776.652893	61.266036
2090.577720	35601.101129	61.271041
2090.203039	35447.482447	61.276046
2089.182379	35272.435060	61.281050
2088.844466	35101.752328	61.286055
2087.927125	34943.419743	61.291060
2087.380215	34775.956548	61.296065
2086.987939	34615.365904	61.301070
2086.114977	34441.536523	61.306074
2085.780117	34270.608936	61.311079
2084.809805	34101.593473	61.316084
2084.443195	33935.157904	61.321089
2083.593985	33758.398732	61.326094
2082.964330	33600.439411	61.331098
2082.414486	33419.391568	61.336103
2081.492067	33253.879108	61.341108
2081.134461	33083.168035	61.346113
2080.507363	32906.401656	61.351118
2079.100789	32743.562759	61.356122
2078.838569	32570.411410	61.361127
2077.720455	32429.152195	61.366132
2077.445135	32253.424163	61.371137
2076.787015	32085.060791	61.376142
2075.819971	31911.838567	61.381146
2075.362172	31762.116436	61.386151
2074.748213	31601.011821	61.391156
2074.396252	31424.279270	61.396161
2073.824986	31260.805762	61.401166
2072.683990	31083.882897	61.406170
2072.286711	30915.385805	61.411175
2071.437256	30762.197137	61.416180
2070.918027	30588.443770	61.421185
2069.946634	30427.495864	61.426190
2069.317545	30262.572047	61.431194
2068.882899	30097.753335	61.436199
2068.015459	29941.946077	61.441204
2067.451662	29776.555442	61.446209
2067.154361	29596.798792	61.451214
2066.156650	29448.986170	61.456218
2065.599592	29286.484389	61.461223
2064.967580	29116.060272	61.466228
2064.506951	28941.419305	61.471233
2063.779068	28786.048047	61.476238
2062.582219	28618.519884	61.481242
2062.357877	28445.996916	61.486247
2061.725532	28279.223140	61.491252
2061.068446	28117.543554	61.496257
2060.388620	27946.712732	61.501262
2059.753364	27778.759720	61.506266
2059.176831	27622.144938	61.511271
2058.276390	27449.795146	61.516276
2057.510094	27282.289869	61.521281
2056.987434	27110.728890	61.526286
2056.230761	26949.216577	61.531290
2055.685259	26779.255861	61.536295
2054.720945	26617.753753	61.541300
2054.321647	26451.183774	61.546305
2053.953932	26282.241064	61.551310
2052.918031	26126.434788	61.556314
2052.262949	25955.572127	61.561319
2051.436358	25797.256651	61.566324
2051.042996	25626.697139	61.571329
2050.131052	25459.418735	61.576334
2049.375914	25306.244499	61.581338
2048.802478	25146.269143	61.586343
2048.239432	24983.638597	61.591348
2047.118313	24816.864468	61.596353
2046.713133	24661.745479	61.601358
2045.636851	24501.813718	61.606362
2045.091232	24346.443672	61.611367
2044.376192	24196.107205	61.616372
2043.795626	24030.157351	61.621377
2043.478272	23879.658880	61.626382
2042.544538	23732.408923	61.631386
2042.339852	23571.299461	61.636391
2041.276051	23426.782362	61.641396
2040.636329	23255.181701	61.646401
2040.137321	23096.503801	61.651406
2039.532505	22939.301967	61.656410
2039.006252	22777.062372	61.661415
2037.843325	22619.581938	61.666420
2037.264214	22467.679128	61.671425
2036.792151	22304.327925	61.676430
2035.951656	22157.289392	61.681434
2035.465741	21996.249224	61.686439
2034.651625	21841.026021	61.691444
2034.003177	21680.839194	61.696449
2033.516198	21532.637839	61.701454
2032.527075	21369.151746	61.706458
2032.302935	21217.626235	61.711463
2031.235459	21072.591147	61.716468
2030.753488	20907.478667	61.721473
2030.080364	20747.343133	61.726478
2029.142573	20603.917837	61.731482
2029.062969	20432.105341	61.736487
2028.164364	20284.131461	61.741492
2027.383010	20133.538544	61.746497
2026.991827	19967.300817	61.751502
2026.122474	19814.271562	61.756506
2025.405207	19660.648471	61.761511
2024.591658	19513.398241	61.766516
2023.940156	19346.721698	61.771521
2023.598338	19199.758758	61.776526
2022.366961	19051.559206	61.781530
2022.223173	18886.076037	61.786535
2021.705002	18738.507944	61.791540
2020.782793	18581.545636	61.796545
2019.845943	18428.093842	61.801550
2019.277276	18279.822492	61.806554
2018.983203	18124.693629	61.811559
2017.883554	17974.412007	61.816564
2017.316690	17822.802802	61.821569
2016.543870	17675.588318	61.826574
2015.504151	17523.598843	61.831578
2015.202069	17371.279469	61.836583
2014.291793	17231.194342	61.841588
2013.289157	17070.379946	61.846593
2012.920823	16935.623871	61.851598
2012.071666	16795.131799	61.856602
2011.693875	16651.045376	61.861607
2010.299050	16533.962705	61.866612
2010.074203	16377.990595	61.871617
2009.548847	16233.304173	61.876622
2008.616881	16104.354072	61.881626
2008.452013	15955.906658	61.886631
2007.735864	15820.072011	61.891636
2006.880908	15684.688876	61.896641
2005.976429	15548.376737	61.901646
2004.995772	15397.341871	61.906650
2004.600046	15269.882604	61.911655
2003.487774	15139.556812	61.916660
2002.845528	15003.264806	61.921665
2002.141131	14876.454560	61.926670
2001.326472	14757.296141	61.931674
2000.691090	14636.776494	61.936679
1999.784304	14511.504176	61.941684
1999.187755	14388.826058	61.946689
1998.346481	14279.512955	61.951694
1997.316398	14155.515593	61.956698
1996.988780	14028.275120	61.961703
1995.935862	13928.308278	61.966708
1995.087886	13825.446491	61.971713
1994.407502	13720.234952	61.976718
1993.124761	13629.776303	61.981722
1992.840743	13529.275614	61.986727
1991.649931	13437.166799	61.991732
1990.960058	13355.702066	61.996737
1989.929186	13274.090166	62.001742
1988.751724	13197.909847	62.006746
1988.204259	13117.386454	62.011751
1986.994137	13054.599975	62.016756
1986.142736	12982.550276	62.021761
1985.199823	12922.144405	62.026766
1984.432526	12865.267539	62.031770
1983.806284	12808.867624	62.036775
1982.932454	12767.098657	62.041780
1982.162496	12691.858983	62.046785
1981.489311	12643.093665	62.051790
1980.735862	12601.381803	62.056794
1980.411933	12548.326720	62.061799
1979.729006	12519.939835	62.066804
1978.766713	12457.835970	62.071809
1978.488556	12407.660107	62.076814
1978.135702	12357.347520	62.081818
1977.374210	12312.908193	62.086823
1976.897052	12257.307534	62.091828
1976.304273	12195.713652	62.096833
1975.716563	12146.988838	62.101838
1974.784815	12095.306213	62.106842
1974.505264	12038.540662	62.111847
1973.398447	11987.524769	62.116852
1973.114120	11933.020526	62.121857
1972.773290	11881.321968	62.126862
1971.898698	11829.611649	62.131866
1971.487883	11766.288773	62.136871
1970.512428	11714.259697	62.141876
1970.122368	11649.378547	62.146881
1969.732201	11603.963090	62.151886
1968.602477	11549.739607	62.156890
1968.262342	11477.085849	62.161895
1967.484314	11424.792671	62.166900
1966.415240	11364.618982	62.171905
1966.176509	11310.159058	62.176910
1965.176645	11255.951920	62.181914
1964.598386	11197.343405	62.186919
1963.843517	11148.593895	62.191924
1963.551598	11095.665260	62.196929
1963.135376	11028.748677	62.201934
1962.496591	10989.022888	62.206938
1962.004366	10923.341848	62.211943
1961.043695	10870.186395	62.216948
1960.781296	10801.800891	62.221953
1960.021999	10750.456082	62.226958
1958.962173	10686.946441	62.231962
1958.524535	10630.090742	62.236967
1957.512369	10578.427854	62.241972
1956.981202	10523.845967	62.246977
1956.482803	10459.459939	62.251982
1955.887320	10407.711768	62.256986
1955.267317	10342.072478	62.261991
1954.479115	10286.016574	62.266996
1953.701010	10225.876598	62.272001
1953.260153	10158.985930	62.277006
1952.626803	10119.814658	62.282010
1951.891559	10057.621505	62.287015
1951.288981	9997.980044	62.292020
1950.835785	9946.063727	62.297025
1950.380005	9876.900065	62.302030
1948.945601	9832.023372	62.307034
1948.779748	9765.547617	62.312039
1947.923972	9710.473844	62.317044
1947.267289	9644.447752	62.322049
1946.430911	9594.234929	62.327054
1945.571532	9547.756148	62.332058
1945.404025	9484.416454	62.337063
1944.752932	9439.818962	62.342068
1944.005191	9384.803793	62.347073
1943.222300	9318.938418	62.352078
1942.759290	9260.773583	62.357082
1942.148918	9201.180705	62.362087
1941.493482	9142.025586	62.367092
1940.772320	9083.491380	62.372097
1940.448929	9024.181453	62.377102
1939.484240	8971.754845	62.382106
1938.900102	8912.896603	62.387111
1938.114484	8859.925210	62.392116
1937.547793	8793.315029	62.397121
1937.091145	8742.346979	62.402126
1936.025744	8682.590145	62.407130
1935.488499	8619.927756	62.412135
1934.845139	8570.536206	62.417140
1934.390800	8515.462271	62.422145
1933.791941	8452.804052	62.427150
1932.895488	8397.894220	62.432154
1932.495564	8336.318841	62.437159
1931.547276	8283.406478	62.442164
1931.083468	8216.557303	62.447169
1930.382603	8160.968823	62.452174
1929.767687	8111.464225	62.457178
1929.180180	8048.444195	62.462183
1928.508824	7986.126435	62.467188
1927.498140	7926.971776	62.472193
1926.525016	7871.289543	62.477198
1926.278071	7823.174286	62.482202
1925.313204	7764.332493	62.487207
1924.731254	7710.971150	62.492212
1924.187697	7651.100503	62.497217
1923.631668	7593.325715	62.502222
1922.848930	7549.825251	62.507226
1922.496188	7476.557802	62.512231
1921.365575	7423.058585	62.517236
1920.949748	7365.719956	62.522241
1920.477987	7317.827399	62.527246
1919.830341	7261.975084	62.532250
1919.438060	7201.952856	62.537255
1918.922799	7137.830297	62.542260
1918.027009	7088.918775	62.547265
1917.588846	7020.632056	62.552270
1916.580822	6971.889404	62.557274
1915.848990	6905.465718	62.562279
1914.989702	6846.087810	62.567284
1914.475676	6785.722154	62.572289
1913.919869	6743.234789	62.577294
1913.071968	6666.000945	62.582298
1912.600027	6612.825647	62.587303
1911.523438	6557.881004	62.592308
1911.203981	6497.085707	62.597313
1910.751583	6431.111996	62.602318
1909.951461	6382.331179	62.607322
1909.381996	6318.251526	62.612327
1908.348120	6271.439153	62.617332
1907.698034	6206.931846	62.622337
1907.235764	6162.158799	62.627342
1906.475984	6109.536614	62.632346
1906.002553	6042.477084	62.637351
1905.297936	5998.384285	62.642356
1904.657668	5932.714746	62.647361
1903.939237	5880.316345	62.652366
1903.053969	5821.842710	62.657370
1902.932801	5766.177470	62.662375
1902.250774	5712.150608	62.667380
1901.274553	5643.404305	62.672385
1900.671329	5581.998411	62.677390
1899.674033	5527.157014	62.682394
1899.385216	5464.165994	62.687399
1898.164079	5427.412602	62.692404
1897.507059	5365.402505	62.697409
1896.954584	5314.868014	62.702414
1896.338954	5267.312531	62.707418
1896.140041	5216.207988	62.712423
1895.213324	5163.371959	62.717428
1894.641361	5109.400026	62.722433
1894.228343	5057.276282	62.727438
1893.039884	4989.751389	62.732442
1892.902307	4926.610876	62.737447
1891.916415	4893.780056	62.742452
1891.511440	4835.705731	62.747457
1890.782292	4761.701443	62.752462
1889.948467	4710.664749	62.757466
1888.998338	4657.280580	62.762471
1888.811166	4606.449964	62.767476
1888.199018	4544.345495	62.772481
1887.119355	4494.363638	62.777486
1886.248293	4463.073228	62.782490
1886.229932	4387.929511	62.787495
1885.356314	4346.208533	62.792500
1884.566212	4278.130732	62.797505
1883.955397	4227.724381	62.802510
1883.493740	4174.689512	62.807514
1882.714248	4119.171279	62.812519
1881.790662	4079.158592	62.817524
1881.415771	4014.748886	62.822529
1880.973457	3972.238861	62.827534
1880.145070	3905.592411	62.832538
1879.687161	3854.364147	62.837543
1878.800634	3811.739778	62.842548
1878.300243	3748.982900	62.847553
1877.637713	3686.768600	62.852558
1876.523837	3632.142850	62.857562
1876.171559	3568.958647	62.862567
1875.733169	3528.618064	62.867572
1874.970476	3468.250250	62.872577
1874.292843	3405.302951	62.877582
1873.190141	3360.542310	62.882586
1872.843703	3295.368630	62.887591
1872.037225	3255.951580	62.892596
1871.355798	3198.777758	62.897601
1870.767375	3154.356433	62.902606
1869.982586	3088.940974	62.907610
1869.659856	3034.519122	62.912615
1868.491239	2973.354263	62.917620
1867.971359	2934.590501	62.922625
1867.752185	2870.712333	62.927630
1866.702768	2825.550568	62.932634
1866.163570	2772.522041	62.937639
1865.257118	2729.120122	62.942644
1864.656899	2679.598283	62.947649
1864.313171	2619.686348	62.952654
1863.536636	2574.795895	62.957658
1862.934117	2512.595195	62.962663
1861.939865	2476.599427	62.967668
1861.501273	2415.488966	62.972673
1860.967421	2363.724388	62.977678
1859.858941	2323.534530	62.982682
1859.310097	2272.100706	62.987687
1858.817754	2220.286675	62.992692
1858.201940	2160.225048	62.997697
1857.287295	2108.793105	63.002702
1856.982122	2056.435001	63.007706
1856.275972	2008.227085	63.012711
1855.278135	1970.896525	63.017716
1854.501351	1909.669974	63.022721
1854.222051	1854.199206	63.027726
1853.512571	1812.927018	63.032730
1853.098881	1767.626592	63.037735
1852.330141	1719.736316	63.042740
1851.533963	1666.771537	63.047745
1851.082214	1621.298610	63.052750
1850.170501	1567.989807	63.057754
1849.592343	1521.848078	63.062759
1848.533127	1469.983999	63.067764
1848.091377	1414.352240	63.072769
1847.719326	1357.616727	63.077774
1846.598665	1312.414990	63.082778
1846.015556	1266.336365	63.087783
1845.118958	1208.839424	63.092788
1845.086596	1174.222308	63.097793
1844.085639	1124.953899	63.102798
1843.651587	1085.672837	63.107802
1843.002710	1025.437421	63.112807
1842.135296	993.416633	63.117812
1841.354524	936.487454	63.122817
1840.542567	896.959392	63.127822
1839.364779	842.001014	63.132826
1839.037497	806.416014	63.137831
1838.190805	767.915715	63.142836
1837.804022	735.413894	63.147841
1836.991754	688.927203	63.152846
1836.679870	648.058830	63.157850
1836.161216	610.743212	63.162855
1835.279126	568.683524	63.167860
1834.715755	519.519584	63.172865
1834.238438	473.694763	63.177870
1833.215241	429.637800	63.182874
1832.687327	377.142916	63.187879
1831.874877	346.529359	63.192884
1831.393896	310.003316	63.197889
1830.753875	266.296013	63.202894
1829.494784	240.123298	63.207898
1829.038143	189.120598	63.212903
1828.387806	152.978229	63.217908
1827.191713	116.589882	63.222913
1826.878792	87.901822	63.227918
1826.197773	61.569835	63.232922
1825.320005	25.501746	63.237927
1824.669741	-0.775088	63.242932
1823.851135	-31.315902	63.247937
1823.133397	-46.765941	63.252942
1822.132805	-75.191520	63.257946
1819.447682	-46.295724	63.262951
1816.786076	14.205520	63.267956
1816.668523	14.159567	63.272961
1817.449206	9.454710	63.277966
1817.203567	11.939536	63.282970
1817.537811	7.682454	63.287975
1816.937380	13.543013	63.292980
1816.321140	11.644535	63.297985
1815.484767	9.963934	63.302990
1814.177802	20.470306	63.307994
1813.696924	16.221236	63.312999
1812.875461	21.823593	63.318004
1811.822240	19.772160	63.323009
1811.164489	18.618268	63.328014
1810.997305	18.534466	63.333018
1810.604979	26.265316	63.338023
1809.772674	23.447117	63.343028
1809.019768	22.215297	63.348033
1808.341681	18.314503	63.353038
1807.454382	27.951594	63.358042
1807.728322	18.645353	63.363047
1807.197535	27.244992	63.368052
1806.292923	22.706828	63.373057
1804.966513	27.982531	63.378062
1803.997945	27.097188	63.383066
1803.944389	27.105726	63.388071
1803.727124	33.271292	63.393076
1802.988004	27.989353	63.398081
1802.736320	18.530045	63.403086
1801.572752	26.470099	63.408090
1800.859562	21.712310	63.413095
1800.121322	37.505651	63.418100
1799.273812	29.216408	63.423105
1798.822669	16.677530	63.428110
1798.114864	27.410456	63.433114
1797.696924	31.723480	63.438119
1796.777967	27.250673	63.443124
1796.140727	36.162106	63.448129
1795.694240	26.533461	63.453134
1794.719103	23.261722	63.458138
1794.370252	24.879872	63.463143
1793.415478	19.370419	63.468148
1792.924281	30.242409	63.473153
1792.309780	30.843062	63.478158
1791.493081	31.278711	63.483162
1791.033221	29.498902	63.488167
1790.625268	28.038847	63.493172
1789.613666	27.221843	63.498177
1789.056138	30.429544	63.503182
1788.063849	33.319946	63.508186
1787.862118	28.421014	63.513191
1787.164653	27.300242	63.518196
1786.440742	24.598874	63.523201
1786.295681	21.504393	63.528206
1784.552191	29.191206	63.533210
1783.880676	19.241923	63.538215
1783.697215	27.081528	63.543220
1783.502180	35.673585	63.548225
1782.639888	26.308090	63.553230
1781.332050	29.272259	63.558234
1780.922852	30.360691	63.563239
1780.678407	28.024717	63.568244
1780.046884	33.358809	63.573249
1779.082204	19.381347	63.578254
1778.105310	34.488786	63.583258
1777.521201	28.305475	63.588263
1777.005456	25.474860	63.593268
1776.840078	36.392881	63.598273
1776.063042	24.118642	63.603278
1774.957313	34.900579	63.608282
1774.673454	28.885623	63.613287
1774.166573	35.023070	63.618292
1773.308636	28.471673	63.623297
1773.327034	18.945825	63.628302
1771.849107	29.837329	63.633306
1771.572202	21.999940	63.638311
1770.516383	31.813611	63.643316
1769.588493	24.360296	63.648321
1769.304701	20.125666	63.653326
1768.270276	28.012108	63.658330
1768.349177	21.305628	63.663335
1767.334470	27.299800	63.668340
1766.647245	25.116147	63.673345
1765.977457	25.113745	63.678350
1765.248895	25.894940	63.683354
1764.761195	26.019735	63.688359
1764.292838	23.571094	63.693364
1763.679760	28.421300	63.698369
1763.281445	20.559043	63.703374
1762.122322	32.822294	63.708378
1761.543347	21.448564	63.713383
1760.377541	31.427934	63.718388
1759.590161	26.883785	63.723393
1759.399386	33.420449	63.728398
1758.962489	32.439647	63.733402
1758.595051	29.408867	63.738407
1757.794761	30.143111	63.743412
1757.054250	29.201066	63.748417
1756.749160	31.168654	63.753422
1755.061887	30.064743	63.758426
1754.380224	22.652753	63.763431
1754.020216	36.354968	63.768436
1753.279957	25.115659	63.773441
1753.172386	19.348672	63.778446
1752.024238	34.379239	63.783450
1751.831151	38.839481	63.788455
1751.314899	28.840315	63.793460
1751.086305	29.294535	63.798465
1749.772523	27.410663	63.803470
1748.416696	29.579821	63.808474
1747.784698	29.636075	63.813479
1747.044076	23.969629	63.818484
1747.048337	35.237587	63.823489
1746.852721	26.136800	63.828494
1745.863475	42.269630	63.833498
1745.572168	22.768546	63.838503
1744.542274	27.781146	63.843508
1743.512775	28.477683	63.848513
1742.952715	20.261083	63.853518
1742.042396	31.833561	63.858522
1741.577668	19.651662	63.863527
1740.955678	34.423628	63.868532
1740.367331	26.817052	63.873537
1740.175941	27.487708	63.878542
1739.334913	27.331166	63.883546
1739.032628	27.592092	63.888551
1737.343511	30.848643	63.893556
1736.716954	22.735643	63.898561
1736.448197	23.169435	63.903566
1735.276641	32.230390	63.908570
1735.128902	25.195640	63.913575
1734.674812	37.328004	63.918580
1733.852725	35.869080	63.923585
1733.587884	35.971100	63.928590
1732.634203	32.539862	63.933594
1731.875897	25.199974	63.938599
1730.960019	27.280341	63.943604
1730.536157	30.922551	63.948609
1730.200928	25.814602	63.953614
1728.977467	33.426739	63.958618
1728.919609	26.324098	63.963623
1728.014495	21.447010	63.968628
1726.743487	30.902221	63.973633
1726.415077	22.311374	63.978638
1725.613702	26.210656	63.983642
1725.448850	22.748750	63.988647
1724.856843	30.728936	63.993652
1724.127081	27.435598	63.998657
1723.977845	27.659602	64.003662
1722.367698	30.236587	64.008666
1721.874133	30.152592	64.013671
1721.182785	23.987909	64.018676
1720.531242	30.850063	64.023681
1720.464744	32.492760	64.028686
1719.385430	32.497070	64.033690
1718.690202	14.209729	64.038695
1717.888142	24.806252	64.043700
1717.272935	32.564627	64.048705
1716.788298	21.466080	64.053710
1716.043637	28.382445	64.058714
1715.625101	24.643874	64.063719
1714.272365	31.950129	64.068724
1713.204933	24.586810	64.073729
1713.722007	25.066094	64.078734
1712.946133	25.236670	64.083738
1712.356963	19.055763	64.088743
1711.839487	22.318615	64.093748
1710.816052	19.783114	64.098753
1709.929732	16.435805	64.103758
1708.923816	29.010617	64.108762
1708.119662	26.087059	64.113767
1707.646965	23.044625	64.118772
1707.387119	25.594793	64.123777
1707.188198	25.317349	64.128782
1706.466663	23.989116	64.133786
1706.044147	21.353439	64.138791
1705.149843	23.313697	64.143796
1704.214548	22.143994	64.148801
1703.802026	17.425211	64.153806
1702.865367	27.658353	64.158810
1702.125068	31.182099	64.163815
1701.113837	32.632667	64.168820
1700.198629	38.972173	64.173825
1699.824538	24.508289	64.178830
1699.416133	28.483928	64.183834
1698.946157	21.363177	64.188839
1698.646515	25.208001	64.193844
1697.889499	26.755382	64.198849
1697.372202	16.158758	64.203854
1696.190872	35.550032	64.208858
1695.408220	28.739134	64.213863
1695.038123	27.504888	64.218868
1694.543870	24.259305	64.223873
1693.939145	19.396016	64.228878
1692.812330	33.276797	64.233882
1692.414797	18.324649	64.238887
1691.767565	25.067851	64.243892
1690.805018	33.638320	64.248897
1690.780841	23.991509	64.253902
1689.679263	21.417969	64.258906
1688.635247	26.079603	64.263911
1687.985083	36.049633	64.268916
1687.392715	26.797419	64.273921
1687.182535	16.905777	64.278926
1686.438040	35.611093	64.283930
1685.978896	28.920695	64.288935
1685.200925	25.664988	64.293940
1684.604853	23.906837	64.298945
1684.049374	15.322111	64.303950
1683.584153	30.275751	64.308954
1682.399348	20.934726	64.313959
1681.532204	22.354528	64.318964
1680.763952	18.080176	64.323969
1680.381892	26.331360	64.328974
1679.708753	27.680923	64.333978
1679.308690	30.909362	64.338983
1678.226433	25.912201	64.343988
1677.177196	24.323804	64.348993
1676.903702	19.683864	64.353998
1676.228421	19.333861	64.359002
1676.019943	20.556000	64.364007
1675.547111	30.928355	64.369012
1675.120012	32.893254	64.374017
1674.201166	26.985491	64.379022
1673.171612	34.759232	64.384026
1672.693171	26.310495	64.389031
1672.215909	34.715575	64.394036
1670.831405	36.118219	64.399041
1669.935277	29.378971	64.404046
1669.467185	39.433621	64.409050
1669.259497	37.610623	64.414055
1668.791066	40.728503	64.419060
1668.335867	33.739444	64.424065
1667.629428	24.751355	64.429070
1666.121810	36.338313	64.434074
1665.686515	27.158922	64.439079
1665.295890	30.434747	64.444084
1664.891661	31.339486	64.449089
1664.246848	32.746053	64.454094
1663.516933	41.967112	64.459098
1662.619269	30.170961	64.464103
1662.027610	28.705418	64.469108
1661.372149	31.356282	64.474113
1660.407989	20.944190	64.479118
1659.522778	35.655478	64.484122
1659.041464	34.736941	64.489127
1658.318384	36.127559	64.494132
1658.022056	27.626242	64.499137
1657.554780	19.733965	64.504142
1657.168791	36.518430	64.509146
1656.444659	26.471895	64.514151
1655.565160	28.839814	64.519156
1654.791700	25.840437	64.524161
1654.433207	25.821728	64.529166
1652.857666	28.729137	64.534170
1652.386369	25.711722	64.539175
1651.730039	31.611158	64.544180
1651.103985	27.047726	64.549185
1650.776912	24.780086	64.554190
1650.605990	18.848137	64.559194
1650.017521	21.322784	64.564199
1648.759326	22.987639	64.569204
1647.927770	29.187716	64.574209
1647.759785	25.021436	64.579214
1646.765622	32.259720	64.584218
1646.050262	27.639516	64.589223
1645.091123	22.201779	64.594228
1644.604207	40.405729	64.599233
1644.297911	29.662055	64.604238
1643.583242	24.634901	64.609242
1643.029240	36.420451	64.614247
1642.034156	26.472157	64.619252
1641.271651	29.967907	64.624257
1641.064305	27.069407	64.629262
1640.562267	27.213848	64.634266
1639.647112	27.859145	64.639271
1638.564459	23.306755	64.644276
1637.787046	28.922661	64.649281
1637.455777	26.849648	64.654286
1636.906051	27.845312	64.659290
1636.948515	26.554997	64.664295
1635.719217	29.953021	64.669300
1634.744093	28.349714	64.674305
1634.372750	23.655940	64.679310
1633.849855	36.806882	64.684314
1633.105733	24.937472	64.689319
1632.224941	23.897906	64.694324
1631.670231	22.538462	64.699329
1631.255386	24.771071	64.704334
1630.568849	29.388551	64.709338
1629.620372	21.000310	64.714343
1628.915767	23.816677	64.719348
1628.170648	22.192602	64.724353
1628.157503	13.862348	64.729358
1627.128653	22.943240	64.734362
1626.247960	22.430347	64.739367
1625.594348	23.155520	64.744372
1625.016900	16.542282	64.749377
1624.415130	21.321331	64.754382
1623.098811	26.945586	64.759386
1622.934386	23.020011	64.764391
1622.355211	26.492948	64.769396
1621.629633	19.534246	64.774401
1621.634678	23.389017	64.779406
1620.471046	29.961968	64.784410
1619.575053	21.645815	64.789415
1618.908971	20.818140	64.794420
1618.204653	22.038635	64.799425
1618.186923	21.899563	64.804430
1617.397901	40.309199	64.809434
1616.638305	23.454493	64.814439
1615.763632	28.202788	64.819444
1615.171040	29.694108	64.824449
1614.429110	13.413756	64.829454
1613.382873	34.708988	64.834458
1612.944427	19.378599	64.839463
1612.164567	29.537969	64.844468
1611.794497	20.524848	64.849473
1611.504533	21.162289	64.854478
1610.817570	28.435353	64.859482
1609.712312	13.141525	64.864487
1609.133339	31.293859	64.869492
1608.638586	31.129652	64.874497
1608.237661	28.518946	64.879502
1607.021777	31.224167	64.884506
1606.469171	12.548379	64.889511
1606.056522	28.331003	64.894516
1605.207869	17.971549	64.899521
1605.285806	12.596143	64.904526
1603.990919	20.790509	64.909530
1603.292622	14.245363	64.914535
1602.525665	22.942466	64.919540
1601.281102	22.607236	64.924545
1600.597527	24.201321	64.929550
1599.986350	29.732479	64.934554
1600.096314	13.701553	64.939559
1599.284652	25.586380	64.944564
1598.751182	20.804835	64.949569
1598.478372	27.780296	64.954574
1597.581186	28.315522	64.959578
1596.772809	19.100815	64.964583
1596.140857	25.712301	64.969588
1595.477318	26.167830	64.974593
1594.612607	15.402516	64.979598
1593.879559	23.085013	64.984602
1593.405881	23.358994	64.989607
1592.621975	16.218766	64.994612
1591.852878	20.797332	64.999617
1591.294442	14.770847	65.004622
1590.543342	31.206471	65.009626
1590.245261	23.720978	65.014631
1589.883201	18.182094	65.019636
1588.592291	24.914046	65.024641
1588.071961	15.806539	65.029646
1587.134707	31.210482	65.034650
1586.974244	31.901465	65.039655
1586.173687	23.970697	65.044660
1585.117266	11.343561	65.049665
1584.582939	24.707617	65.054670
1584.107343	24.207644	65.059674
1583.728398	16.960501	65.064679
1583.571446	21.030236	65.069684
1582.045688	29.803755	65.074689
1581.851702	8.659912	65.079694
1580.719051	19.701633	65.084698
1579.357748	18.364704	65.089703
1579.324694	11.650794	65.094708
1578.562313	21.684390	65.099713
1578.233446	11.840014	65.104718
1577.050873	19.721665	65.109722
1577.032918	14.344148	65.114727
1576.792904	13.906091	65.119732
1575.378209	20.269795	65.124737
1574.569983	18.472843	65.129742
1573.582793	11.585690	65.134746
1573.465115	7.693697	65.139751
1573.149137	11.861235	65.144756
1572.330177	22.622890	65.149761
1571.473117	12.898708	65.154766
1570.767142	21.959853	65.159770
1570.068229	25.290979	65.164775
1569.761842	24.871353	65.169780
1568.926937	19.470679	65.174785
1568.294656	16.215520	65.179790
1567.407663	15.258961	65.184794
1567.359756	14.293656	65.189799
1566.372155	12.454247	65.194804
1565.435312	30.556213	65.199809
1564.778421	19.297432	65.204814
1564.371783	13.740408	65.209818
1563.994601	13.213763	65.214823
1563.019280	19.496622	65.219828
1562.133427	15.621031	65.224833
1561.613440	12.974063	65.229838
1560.897590	28.380674	65.234842
1560.639136	20.543550	65.239847
1559.389270	18.878275	65.244852
1558.595716	19.198358	65.249857
1558.385793	17.288999	65.254862
1557.729092	21.311989	65.259866
1557.418078	23.599071	65.264871
1556.445095	19.579635	65.269876
1555.508208	27.296107	65.274881
1555.214277	20.465956	65.279886
1554.519669	20.497514	65.284890
1553.922676	24.083677	65.289895
1553.112610	17.814919	65.294900
1552.037703	19.923767	65.299905
1552.068851	21.464219	65.304910
1551.495810	15.466874	65.309914
1550.352124	26.839936	65.314919
1549.564271	22.324321	65.319924
1549.034477	21.574354	65.324929
1548.802872	21.503959	65.329934
1547.202717	32.473332	65.334938
1546.415269	29.234947	65.339943
1546.208713	19.148795	65.344948
1545.645328	22.141433	65.349953
1545.621354	17.201677	65.354958
1544.716191	24.752266	65.359962
1543.964084	17.640118	65.364967
1543.185978	12.687734	65.369972
1542.553720	14.541751	65.374977
1542.429456	14.460608	65.379982
1541.056469	23.324982	65.384986
1540.842901	21.392550	65.389991
1540.227872	20.741281	65.394996
1539.162967	20.259266	65.400001
1538.520828	15.389354	65.405006
1537.274162	28.415612	65.410010
1537.024955	19.668725	65.415015
1536.321993	21.322674	65.420020
1535.761241	24.109898	65.425025
1535.445539	19.300074	65.430030
1534.528836	24.575448	65.435034
1533.706901	14.740047	65.440039
1533.462471	22.967790	65.445044
1532.792608	28.492516	65.450049
1532.329710	22.055061	65.455054
1531.139843	14.269758	65.460058
1530.908044	28.191279	65.465063
1530.117005	32.394892	65.470068
1529.167545	27.777234	65.475073
1528.859885	18.872485	65.480078
1528.008753	29.123618	65.485082
1527.884740	18.753126	65.490087
1526.562809	30.531402	65.495092
1525.696372	29.238863	65.500097
1525.308152	20.152957	65.505102
1524.820174	32.516208	65.510106
1524.076072	19.645509	65.515111
1523.122858	30.707626	65.520116
1522.377909	30.923806	65.525121
1522.125246	24.973323	65.530126
1521.249322	23.202914	65.535130
1520.927378	23.556873	65.540135
1519.907725	26.098488	65.545140
1519.311673	24.759832	65.550145
1518.943925	21.916797	65.555150
1518.340972	26.074754	65.560154
1517.312990	26.993481	65.565159
1516.699636	22.721376	65.570164
1515.946614	23.432412	65.575169
1515.913499	19.318831	65.580174
1514.487259	31.698721	65.585178
1513.762245	31.566392	65.590183
1513.302170	33.979666	65.595188
1512.851479	19.695168	65.600193
1512.705746	24.879571	65.605198
1511.605362	25.729383	65.610202
1510.997940	23.676621	65.615207
1510.235572	21.840864	65.620212
1509.527876	27.770564	65.625217
1508.616126	25.799278	65.630222
1507.658419	28.315285	65.635226
1507.468184	28.337664	65.640231
1506.896888	23.697767	65.645236
1506.367259	26.046402	65.650241
1505.749415	24.307525	65.655246
1504.626491	25.884721	65.660250
1504.565043	26.235131	65.665255
1503.950458	25.774606	65.670260
1502.683218	20.180896	65.675265
1502.144170	29.379529	65.680270
1501.344476	37.635598	65.685274
1501.088682	22.836019	65.690279
1500.468411	20.466766	65.695284
1499.497646	18.034946	65.700289
1498.722632	12.498632	65.705294
1498.060977	26.934724	65.710298
1498.013853	29.164107	65.715303
1497.037969	26.447679	65.720308
1496.130032	20.684912	65.725313
1495.707385	14.871835	65.730318
1494.982965	22.674402	65.735322
1494.465697	26.216368	65.740327
1493.513585	26.607399	65.745332
1492.630417	28.641648	65.750337
1492.753637	24.052228	65.755342
1491.838600	24.126717	65.760346
1490.905743	16.464590	65.765351
1490.234821	25.143300	65.770356
1489.683052	28.870519	65.775361
1489.171240	24.175443	65.780366
1487.849038	25.131477	65.785370
1487.431089	22.165543	65.790375
1487.369754	27.938912	65.795380
1486.919076	21.830676	65.800385
1486.428307	21.251134	65.805390
1484.931721	24.035708	65.810394
1484.629745	19.698360	65.815399
1483.785696	16.521032	65.820404
1482.590033	22.490438	65.825409
1482.436583	12.119905	65.830414
1481.731594	18.501748	65.835418
1481.532917	20.203298	65.840423
1480.426519	28.055537	65.845428
1479.397458	22.968018	65.850433
1478.912138	14.793240	65.855438
1478.275001	22.000061	65.860442
1478.296307	21.056873	65.865447
1477.215611	19.784211	65.870452
1476.254260	28.769271	65.875457
1475.940155	9.959448	65.880462
1475.635173	18.890650	65.885466
1474.561430	19.521784	65.890471
1473.974007	19.671943	65.895476
1473.016505	15.415124	65.900481
1472.603681	10.335330	65.905486
1471.289856	20.549620	65.910490
1470.601717	13.894099	65.915495
1470.476348	19.307069	65.920500
1469.871577	26.538711	65.925505
1469.940661	22.058817	65.930510
1468.342459	12.208048	65.935514
1467.771964	22.728392	65.940519
1467.148581	25.919809	65.945524
1466.667594	19.310210	65.950529
1466.225570	10.737484	65.955534
1465.059071	27.335327	65.960538
1464.805733	10.780284	65.965543
1464.108173	1.699414	65.970548
1463.317954	25.705664	65.975553
1462.520984	2.877374	65.980558
1461.524260	15.988499	65.985562
1461.358847	20.677727	65.990567
1461.046604	19.568361	65.995572
1460.134419	23.081637	66.000577
1459.346825	6.545280	66.005582
1458.490781	14.332500	66.010586
1458.161919	17.324149	66.015591
1457.526680	19.937150	66.020596
1456.748197	11.329594	66.025601
1456.252573	12.065967	66.030606
1455.497851	19.569013	66.035610
1454.428899	23.100899	66.040615
1453.647211	16.895476	66.045620
1453.020013	20.380805	66.050625
1452.734483	12.940657	66.055630
1452.071009	16.193638	66.060634
1451.672002	17.564341	66.065639
1450.827107	30.239778	66.070644
1449.904205	18.458788	66.075649
1449.549211	9.594700	66.080654
1448.942904	24.871949	66.085658
1448.046993	15.631796	66.090663
1447.492312	18.441724	66.095668
1446.941630	22.640270	66.100673
1446.401904	12.720631	66.105678
1445.069758	21.296288	66.110682
1444.322301	19.745179	66.115687
1443.883101	23.749394	66.120692
1443.533340	34.269358	66.125697
1443.407855	21.909056	66.130702
1442.066279	27.449100	66.135706
1441.610752	14.647690	66.140711
1441.200808	24.573259	66.145716
1440.212326	18.602552	66.150721
1439.891359	5.357154	66.155726
1438.864147	27.073567	66.160730
1438.178429	21.956727	66.165735
1437.428316	15.803061	66.170740
1436.804694	25.144446	66.175745
1436.682562	11.435369	66.180750
1435.446847	28.468409	66.185754
1434.635160	23.844662	66.190759
1434.163104	23.721035	66.195764
1433.623612	22.827559	66.200769
1433.317494	11.292315	66.205774
1431.965114	22.187664	66.210778
1431.535470	24.794802	66.215783
1430.867644	21.151103	66.220788
1430.617736	20.583750	66.225793
1429.480510	19.324824	66.230798
1428.566326	21.837094	66.235802
1428.274500	19.672692	66.240807
1427.864454	25.471522	66.245812
1426.894594	23.678232	66.250817
1426.088180	26.025145	66.255822
1425.282115	28.471347	66.260826
1425.264953	22.548103	66.265831
1424.813020	26.710458	66.270836
1423.151537	28.571980	66.275841
1423.119634	21.419517	66.280846
1422.420780	19.581577	66.285850
1422.160156	19.149965	66.290855
1421.148807	23.849077	66.295860
1420.102358	32.753067	66.300865
1419.531815	18.218001	66.305870
1419.276522	24.600919	66.310874
1418.214780	18.870517	66.315879
1417.676734	22.081494	66.320884
1416.926371	31.977602	66.325889
1416.909777	22.094661	66.330894
1415.874397	17.996896	66.335898
1415.016143	25.816022	66.340903
1414.423210	15.474354	66.345908
1414.017904	30.893122	66.350913
1413.147170	24.774402	66.355918
1411.890813	35.574085	66.360922
1411.382028	13.089496	66.365927
1411.316888	17.855823	66.370932
1410.637399	23.350563	66.375937
1409.801142	20.832745	66.380942
1409.102061	25.639917	66.385946
1408.559268	9.433666	66.390951
1408.136873	11.087204	66.395956
1406.990845	29.645054	66.400961
1406.595684	21.664112	66.405966
1406.095993	17.673586	66.410970
1405.164831	20.723131	66.415975
1404.186978	16.400192	66.420980
1403.378976	25.693622	66.425985
1403.157073	21.212676	66.430990
1402.785356	22.990620	66.435994
1402.492737	20.249201	66.440999
1401.432850	15.623923	66.446004
1400.657827	28.296146	66.451009
1399.814422	16.858925	66.456014
1398.696225	28.071871	66.461018
1398.234636	11.034302	66.466023
1397.780847	16.901584	66.471028
1397.118949	18.783999	66.476033
1396.968902	18.285928	66.481038
1396.070097	15.803289	66.486042
1395.287492	23.886352	66.491047
1394.998213	9.290827	66.496052
1394.042127	18.596755	66.501057
1393.438956	23.904331	66.506062
1392.595362	17.781309	66.511066
1392.116658	16.786719	66.516071
1391.109108	12.962078	66.521076
1390.292505	22.381450	66.526081
1389.947687	20.034672	66.531086
1389.231089	22.395702	66.536090
1389.149175	11.055058	66.541095
1388.226306	18.450810	66.546100
1386.943015	25.142213	66.551105
1387.011965	20.187695	66.556110
1386.012166	20.173197	66.561114
1384.898991	21.465051	66.566119
1384.529838	28.731791	66.571124
1383.948040	20.936637	66.576129
1383.651963	13.577023	66.581134
1383.020026	25.341860	66.586138
1382.085105	17.582341	66.591143
1381.317672	17.675983	66.596148
1380.805221	28.198152	66.601153
1380.162489	22.861616	66.606158
1378.855127	26.461389	66.611162
1378.328706	16.008239	66.616167
1377.871354	16.834734	66.621172
1377.219974	25.860429	66.626177
1377.340862	24.653838	66.631182
1376.263359	30.274933	66.636186
1375.775771	21.130745	66.641191
1375.188933	20.408806	66.646196
1373.635692	32.741137	66.651201
1373.250719	21.869696	66.656206
1372.388277	30.233532	66.661210
1372.096566	29.314872	66.666215
1372.183798	25.163244	66.671220
1370.893193	19.606436	66.676225
1370.252581	17.946905	66.681230
1369.495994	27.741510	66.686234
1369.156910	26.082929	66.691239
1368.376087	17.439508	66.696244
1367.297423	23.065519	66.701249
1367.057760	23.266072	66.706254
1365.938000	30.426639	66.711258
1365.425604	19.255347	66.716263
1364.905669	21.367507	66.721268
1363.921185	26.906011	66.726273
1363.990786	19.707458	66.731278
1362.888820	24.119806	66.736282
1362.185740	23.567732	66.741287
1361.551364	14.998802	66.746292
1361.200338	23.405913	66.751297
1360.139038	24.501880	66.756302
1359.523302	28.616169	66.761306
1358.893321	20.846028	66.766311
1358.319296	20.653472	66.771316
1357.585880	18.992929	66.776321
1356.757149	19.194090	66.781326
1355.997809	22.735138	66.786330
1355.775004	17.256164	66.791335
1355.104633	18.025066	66.796340
1354.559701	23.980959	66.801345
1353.909558	17.043479	66.806350
1353.131462	24.233307	66.811354
1352.482713	23.869711	66.816359
1351.413353	23.024219	66.821364
1350.708261	36.765518	66.826369
1350.498715	14.309076	66.831374
1349.890585	19.360412	66.836378
1349.039220	26.654928	66.841383
1348.803659	20.687564	66.846388
1348.099390	23.284757	66.851393
1347.137283	23.608046	66.856398
1345.927210	22.203049	66.861402
1345.430591	13.271615	66.866407
1345.207491	20.042064	66.871412
1344.519172	29.488364	66.876417
1343.723123	20.576144	66.881422
1342.879336	20.164712	66.886426
1342.199787	23.158509	66.891431
1341.962958	23.468997	66.896436
1341.214669	20.924603	66.901441
1340.480782	19.495944	66.906446
1339.541487	22.519997	66.911450
1339.490294	19.837974	66.916455
1338.456381	25.553073	66.921460
1337.228644	23.138517	66.926465
1337.339512	18.467487	66.931470
1336.841911	25.325731	66.936474
1335.840901	25.216830	66.941479
1335.030587	15.064286	66.946484
1334.391894	29.960356	66.951489
1334.258695	20.770877	66.956494
1333.346240	16.658338	66.961498
1332.117899	18.326480	66.966503
1331.762587	20.325744	66.971508
1331.312186	28.203050	66.976513
1331.303911	11.935502	66.981518
1329.609054	22.685074	66.986522
1329.058613	20.407265	66.991527
1328.670274	20.404384	66.996532
1328.053479	21.995803	67.001537
1327.131972	8.732371	67.006542
1326.703931	22.415422	67.011546
1326.118581	22.852281	67.016551
1325.234622	20.263232	67.021556
1324.145772	19.523348	67.026561
1323.889489	11.556622	67.031566
1323.002695	18.861504	67.036570
1322.442874	19.062500	67.041575
1322.145232	12.417485	67.046580
1321.446081	16.141354	67.051585
1321.062770	13.508981	67.056590
1320.153707	25.458227	67.061594
1319.481935	10.021545	67.066599
1318.559251	9.781932	67.071604
1317.918791	22.513192	67.076609
1317.589860	19.296604	67.081614
1316.136630	17.394133	67.086618
1315.851227	23.829148	67.091623
1315.105096	19.469406	67.096628
1314.623307	23.556099	67.101633
1314.522052	19.286212	67.106638
1313.353754	19.460952	67.111642
1312.785927	23.176560	67.116647
1312.509241	7.738569	67.121652
1311.164450	21.926905	67.126657
1310.830852	12.794527	67.131662
1310.000672	14.997021	67.136666
1309.563859	22.222482	67.141671
1308.810398	19.724651	67.146676
1307.879921	12.193113	67.151681
1307.643003	11.489671	67.156686
1307.115703	23.851293	67.161690
1306.209709	13.939471	67.166695
1305.650314	16.696560	67.171700
1305.080079	18.532885	67.176705
1304.038619	14.384101	67.181710
1302.911480	17.387570	67.186714
1302.553853	8.757317	67.191719
1302.126729	5.054893	67.196724
1301.673075	3.756728	67.201729
1301.040595	4.513311	67.206734
1300.123303	18.595834	67.211738
1299.406519	14.508967	67.216743
1299.144232	5.177608	67.221748
1298.314073	13.030134	67.226753
1297.516629	5.398608	67.231758
1296.618135	10.242236	67.236762
1296.446308	7.595166	67.241767
1295.327404	19.279743	67.246772
1294.340891	23.063500	67.251777
1293.917181	17.324751	67.256782
1293.452388	15.597864	67.261786
1293.309339	7.766102	67.266791
1293.053306	4.465393	67.271796
1291.395374	15.734217	67.276801
1290.845377	11.776948	67.281806
1290.294291	6.375414	67.286810
1289.108882	22.254085	67.291815
1288.763338	7.762151	67.296820
1288.096550	4.214526	67.301825
1288.163596	3.931095	67.306830
1286.977465	32.702628	67.311834
1286.260673	20.677640	67.316839
1285.639134	4.963341	67.321844
1285.157705	20.432045	67.326849
1284.435155	17.145588	67.331854
1283.296340	26.931598	67.336858
1283.087249	13.245838	67.341863
1282.871062	18.983894	67.346868
1281.899445	17.060060	67.351873
1280.943247	7.891072	67.356878
1280.379766	20.711016	67.361882
1280.005194	11.206705	67.366887
1279.082586	13.729823	67.371892
1277.932811	9.215087	67.376897
1277.637192	20.715152	67.381902
1277.364174	2.928587	67.386906
1276.149659	7.942313	67.391911
1275.228434	15.224296	67.396916
1274.841314	12.365464	67.401921
1274.657418	5.126807	67.406926
1273.918425	19.404905	67.411930
1273.113793	14.206108	67.416935
1272.665862	4.382318	67.421940
1271.761734	19.244896	67.426945
1271.362557	16.085216	67.431950
1270.382305	16.217460	67.436954
1269.949582	18.052427	67.441959
1269.299540	6.614490	67.446964
1268.139800	14.224549	67.451969
1267.514676	5.307268	67.456974
1266.934883	6.996891	67.461978
1266.827263	2.515144	67.466983
1266.280771	5.784255	67.471988
1265.112040	9.712107	67.476993
1264.696684	10.654941	67.481998
1263.930034	5.596763	67.487002
1263.258827	3.970511	67.492007
1262.795740	6.630294	67.497012
1261.674449	17.386465	67.502017
1261.486456	4.615120	67.507022
1260.049202	19.045248	67.512026
1259.595878	18.696331	67.517031
1259.391478	18.400871	67.522036
1258.729359	21.000844	67.527041
1257.872989	8.854574	67.532046
1256.963356	-0.622989	67.537050
1256.531945	15.391248	67.542055
1256.448827	12.198661	67.547060
1255.203671	10.031338	67.552065
1254.507080	7.292680	67.557070
1253.912858	11.108684	67.562074
1253.369288	13.743421	67.567079
1252.968966	8.683763	67.572084
1251.660218	16.826863	67.577089
1251.404915	11.299459	67.582094
1250.953355	8.941294	67.587098
1249.901803	13.273129	67.592103
1249.045105	11.618031	67.597108
1248.461649	20.833208	67.602113
1248.185224	13.874183	67.607118
1247.142218	22.012876	67.612122
1246.064340	8.060015	67.617127
1246.009313	14.338551	67.622132
1245.346566	17.369120	67.627137
1244.994492	-0.064250	67.632142
1244.112191	7.391315	67.637146
1243.520990	12.271248	67.642151
1243.307025	6.065515	67.647156
1242.178058	13.828380	67.652161
1241.427852	8.198333	67.657166
1240.578315	16.828214	67.662170
1240.016675	5.429846	67.667175
1239.127377	13.007949	67.672180
1238.245691	20.826112	67.677185
1237.954020	10.988518	67.682190
1237.020408	20.702486	67.687194
1236.939547	9.155127	67.692199
1236.753124	7.680443	67.697204
1235.413631	18.051866	67.702209
1235.325695	7.934305	67.707214
1233.917274	10.673457	67.712218
1232.961576	13.640230	67.717223
1232.494032	3.389078	67.722228
1232.090686	16.628243	67.727233
1232.155419	12.377700	67.732238
1231.085372	23.277119	67.737242
1230.170235	16.214668	67.742247
1229.641475	16.369745	67.747252
1228.893829	19.968888	67.752257
1227.912155	5.994434	67.757262
1227.102871	18.162786	67.762266
1226.856686	16.848988	67.767271
1226.509837	23.153433	67.772276
1225.814175	25.419715	67.777281
1225.108642	20.974702	67.782286
1224.038488	24.066911	67.787290
1223.624895	18.810677	67.792295
1222.677674	7.803201	67.797300
1221.591384	19.894185	67.802305
1221.707213	4.474226	67.807310
1221.070069	10.995135	67.812314
1220.760044	15.401442	67.817319
1219.807118	19.260305	67.822324
1219.044409	19.755353	67.827329
1218.397942	-1.683822	67.832334
1217.092885	27.368387	67.837338
1216.514008	14.370630	67.842343
1216.555247	4.839637	67.847348
1215.912636	19.061416	67.852353
1215.558770	18.701422	67.857358
1214.233592	18.839656	67.862362
1213.617406	8.519107	67.867367
1213.219681	15.799856	67.872372
1212.039281	24.468172	67.877377
1211.330349	8.562802	67.882382
1210.918656	17.203483	67.887386
1210.882760	12.470642	67.892391
1209.367081	15.261557	67.897396
1209.072052	19.894133	67.902401
1208.676256	14.365424	67.907406
1208.099187	17.256224	67.912410
1206.965606	13.253017	67.917415
1205.996197	14.987268	67.922420
1205.645465	17.968226	67.927425
1205.453499	6.383351	67.932430
1204.003429	12.014867	67.937434
1203.609490	10.505381	67.942439
1203.137478	5.321523	67.947444
1202.416048	19.566877	67.952449
1202.064911	12.029983	67.957454
1200.810840	21.022243	67.962458
1200.093983	9.164462	67.967463
1200.122241	9.390229	67.972468
1199.097172	26.189570	67.977473
1198.275839	16.627019	67.982478
1197.606836	14.625132	67.987482
1197.336862	16.003734	67.992487
1197.023535	13.109527	67.997492
1195.538766	21.302722	68.002497
1195.161395	15.157671	68.007502
1194.511660	20.510533	68.012506
1193.821210	18.220331	68.017511
1192.889648	13.517973	68.022516
1192.150826	20.146522	68.027521
1192.001443	16.504022	68.032526
1191.302948	20.850692	68.037530
1190.450233	14.953122	68.042535
1189.805699	19.269134	68.047540
1189.087330	17.839630	68.052545
1188.833203	11.947785	68.057550
1187.862569	22.541257	68.062554
1187.519845	20.268293	68.067559
1186.845089	15.919320	68.072564
1185.680595	23.735168	68.077569
1184.934589	19.638792	68.082574
1184.100649	24.353924	68.087578
1183.741782	23.029667	68.092583
1183.640354	18.553245	68.097588
1182.971856	16.513436	68.102593
1182.222533	21.180419	68.107598
1181.377135	26.567556	68.112602
1180.998652	12.262232	68.117607
1179.910100	12.799652	68.122612
1179.194548	22.653992	68.127617
1179.049930	14.291077	68.132622
1178.093525	8.383197	68.137626
1177.188190	8.673868	68.142631
1177.175425	12.241298	68.147636
1176.065934	17.312480	68.152641
1175.267648	10.181010	68.157646
1174.240012	25.577324	68.162650
1174.004291	10.410388	68.167655
1173.653327	15.722042	68.172660
1172.155021	21.285558	68.177665
1171.986489	5.838292	68.182670
1171.493211	20.660777	68.187674
1171.149713	14.669612	68.192679
1170.041534	7.924888	68.197684
1168.958515	16.923069	68.202689
1168.775282	11.994476	68.207694
1168.094381	8.431785	68.212698
1167.951657	10.214336	68.217703
1166.893500	16.849524	68.222708
1165.962779	19.815502	68.227713
1165.812732	17.843046	68.232718
1164.466769	27.299356	68.237722
1163.696888	18.701583	68.242727
1163.554041	7.681318	68.247732
1162.940244	19.466943	68.252737
1162.462052	15.813666	68.257742
1161.384096	22.182358	68.262746
1160.775847	15.673503	68.267751
1160.535071	19.341852	68.272756
1159.327796	23.611760	68.277761
1158.822426	12.259657	68.282766
1158.060855	15.258656	68.287770
1157.662211	1.891657	68.292775
1156.501064	21.100066	68.297780
1155.753703	27.345220	68.302785
1155.371754	14.688313	68.307790
1154.853507	13.584946	68.312794
1154.480342	11.141794	68.317799
1153.920968	7.991849	68.322804
1152.778236	23.483740	68.327809
1152.664372	10.033594	68.332814
1151.497562	18.701345	68.337818
1150.496115	13.871353	68.342823
1150.175436	13.614896	68.347828
1149.512160	16.289192	68.352833
1149.419680	8.815247	68.357838
1148.328251	19.043176	68.362842
1147.534294	14.881904	68.367847
1147.143094	16.276638	68.372852
1146.009705	13.984364	68.377857
1145.225871	12.451749	68.382862
1144.766560	18.655818	68.387866
1144.497860	23.211673	68.392871
1144.260617	12.906565	68.397876
1142.931159	11.908574	68.402881
1142.450894	12.120609	68.407886
1141.648605	14.446446	68.412890
1141.024471	12.954661	68.417895
1140.231050	11.757875	68.422900
1139.336001	17.883022	68.427905
1139.106462	4.583743	68.432910
1138.673355	16.290168	68.437914
1137.655061	12.374309	68.442919
1137.078467	5.095636	68.447924
1136.538038	17.285894	68.452929
1135.957161	14.028989	68.457934
1134.937703	23.665180	68.462938
1134.403240	14.451254	68.467943
1134.240857	15.752827	68.472948
1132.808368	18.161559	68.477953
1131.955451	8.171997	68.482958
1131.286353	19.800848	68.487962
1130.997273	15.053092	68.492967
1130.814479	18.201305	68.497972
1129.790549	12.394069	68.502977
1129.186556	13.884151	68.507982
1128.552292	18.545459	68.512986
1127.849092	15.656507	68.517991
1127.029846	10.389130	68.522996
1126.407644	7.309107	68.528001
1125.968293	22.348514	68.533006
1125.367773	24.170771	68.538010
1124.167404	12.875611	68.543015
1123.777592	17.837070	68.548020
1123.311135	20.123687	68.553025
1122.846119	20.848946	68.558030
1121.571066	20.649684	68.563034
1120.758545	20.719038	68.568039
1120.680994	12.932070	68.573044
1119.760095	15.103321	68.578049
1119.134369	17.413696	68.583054
1118.161955	24.640794	68.588058
1118.034109	15.098853	68.593063
1117.604274	9.570849	68.598068
1116.533137	18.516697	68.603073
1115.956612	7.555962	68.608078
1115.204468	17.670011	68.613082
1114.822614	18.656423	68.618087
1113.931506	5.448189	68.623092
1113.282403	22.181433	68.628097
1112.938873	10.276919	68.633102
1111.968168	20.550310	68.638106
1111.049209	16.777928	68.643111
1110.467432	12.573458	68.648116
1109.661505	17.601109	68.653121
1109.804984	12.128562	68.658126
1108.688855	15.709080	68.663130
1107.785801	27.468192	68.668135
1107.402153	24.399108	68.673140
1106.605716	21.261650	68.678145
1105.796871	14.040426	68.683150
1104.958412	14.574364	68.688154
1104.608700	24.443062	68.693159
1104.237162	20.361261	68.698164
1103.051158	28.417098	68.703169
1102.413860	25.484553	68.708174
1101.972431	8.521158	68.713178
1101.727040	21.812471	68.718183
1101.338235	24.107240	68.723188
1100.022664	24.352811	68.728193
1099.628249	20.307766	68.733198
1098.967993	28.056053	68.738202
1097.729937	21.010333	68.743207
1097.163804	19.791597	68.748212
1096.472298	20.466160	68.753217
1096.262291	20.990015	68.758222
1095.677713	17.415175	68.763226
1094.627758	26.693544	68.768231
1094.175381	21.408816	68.773236
1093.580865	18.674467	68.778241
1093.440698	18.556454	68.783246
1092.363577	20.150191	68.788250
1091.470572	27.981234	68.793255
1090.610859	15.692071	68.798260
1089.712261	22.115832	68.803265
1089.408402	10.820003	68.808270
1089.142350	14.620104	68.813274
1088.105190	23.765556	68.818279
1087.224887	13.630561	68.823284
1086.684484	20.508256	68.828289
1086.437449	20.866121	68.833294
1086.346256	24.501218	68.838298
1084.966733	12.370442	68.843303
1084.143212	6.548695	68.848308
1083.267919	24.120564	68.853313
1082.300889	8.729379	68.858318
1081.468844	27.600044	68.863322
1081.290404	23.014460	68.868327
1081.137146	17.388850	68.873332
1080.681728	18.016398	68.878337
1080.084018	9.075896	68.883342
1079.156587	23.413961	68.888346
1078.387638	23.416475	68.893351
1077.103826	15.466601	68.898356
1075.983051	14.736635	68.903361
1075.788405	13.684305	68.908366
1075.714908	21.446480	68.913370
1075.173544	23.661446	68.918375
1074.893914	13.437209	68.923380
1073.861227	24.010622	68.928385
1073.223716	6.143333	68.933390
1072.597111	20.622768	68.938394
1071.904960	19.368894	68.943399
1071.073955	13.253461	68.948404
1070.084348	22.304623	68.953409
1069.615176	11.046136	68.958414
1068.749555	12.248280	68.963418
1067.696125	2.981329	68.968423
1067.592401	28.095752	68.973428
1067.071078	19.788047	68.978433
1066.768626	16.333908	68.983438
1065.797116	19.043067	68.988442
1064.814563	16.846679	68.993447
1064.631184	11.117060	68.998452
1063.779169	20.822823	69.003457
1062.920561	0.321032	69.008462
1062.109214	19.551081	69.013466
1061.873341	15.433515	69.018471
1061.680058	6.162187	69.023476
1060.221970	21.912421	69.028481
1059.808040	21.016399	69.033486
1059.448549	22.369832	69.038490
1058.498292	10.891426	69.043495
1057.870220	17.798840	69.048500
1056.916472	26.470580	69.053505
1056.379047	22.211758	69.058510
1055.172948	22.378438	69.063514
1054.742115	17.427749	69.068519
1054.392496	10.029415	69.073524
1053.800710	23.213414	69.078529
1053.773673	10.692459	69.083534
1052.945946	14.003197	69.088538
1051.922054	13.355597	69.093543
1051.612649	5.026807	69.098548
1050.018425	11.368860	69.103553
1049.630557	8.138042	69.108558
1049.262751	13.472884	69.113562
1048.950485	5.776884	69.118567
1048.194249	19.553149	69.123572
1047.242563	23.347220	69.128577
1046.985536	11.121466	69.133582
1045.430816	15.205431	69.138586
1044.754587	12.299600	69.143591
1043.932154	5.197256	69.148596
1043.235686	22.455262	69.153601
1043.438674	12.674627	69.158606
1043.136790	10.913989	69.163610
1042.238301	18.263382	69.168615
1041.552974	13.088268	69.173620
1040.675370	17.256893	69.178625
1039.996121	11.541514	69.183630
1039.070372	18.174603	69.188634
1038.366583	12.549858	69.193639
1038.688431	7.566158	69.198644
1037.219433	15.482539	69.203649
1036.628650	6.851599	69.208654
1036.419224	14.673239	69.213658
1035.544174	20.587085	69.218663
1034.546878	7.048866	69.223668
1033.465379	11.650463	69.228673
1033.362516	10.140427	69.233678
1033.080779	-2.324223	69.238682
1031.972110	8.213972	69.243687
1031.403431	13.741618	69.248692
1030.694160	20.811762	69.253697
1030.098293	-2.951830	69.258702
1028.829779	19.168867	69.263706
1028.417651	19.396890	69.268711
1028.389598	7.806472	69.273716
1027.510280	9.753526	69.278721
1026.923635	9.138869	69.283726
1026.325379	12.517182	69.288730
1025.424274	-5.683435	69.293735
1025.007739	14.839926	69.298740
1023.536575	4.617630	69.303745
1023.394928	2.524007	69.308750
1022.519001	-3.092262	69.313754
1022.054289	24.897488	69.318759
1021.685945	-3.465837	69.323764
1020.200623	15.855674	69.328769
1020.080314	9.879492	69.333774
1019.603373	11.891835	69.338778
1019.080193	9.770609	69.343783
1018.560864	-4.983731	69.348788
1017.466238	4.859977	69.353793
1016.658275	16.274400	69.358798
1016.083897	16.928771	69.363802
1015.130683	7.920279	69.368807
1015.082418	14.593529	69.373812
1014.234520	25.946508	69.378817
1013.996855	6.739917	69.383822
1012.816864	11.814492	69.388826
1012.231423	11.327375	69.393831
1011.766753	12.099904	69.398836
1010.346908	2.859744	69.403841
1010.052987	3.983561	69.408846
1009.410446	6.564706	69.413850
1009.234690	5.476262	69.418855
1008.593700	10.657460	69.423860
1007.575605	15.950698	69.428865
1007.183141	3.792239	69.433870
1006.555047	17.270585	69.438874
1005.511083	21.596574	69.443879
1005.205298	2.381908	69.448884
1004.306725	7.763356	69.453889
1003.363132	4.702966	69.458894
1002.344790	0.538029	69.463898
1001.727889	15.637218	69.468903
1001.934774	-0.755948	69.473908
1001.161905	21.919809	69.478913
1000.832397	5.897399	69.483918
1000.059677	-0.700343	69.488922
999.162478	5.123995	69.493927
998.081228	12.863585	69.498932
997.362793	18.006650	69.503937
996.758895	5.400880	69.508942
996.356203	4.460505	69.513946
995.893110	7.254366	69.518951
994.995351	12.730302	69.523956
994.447587	17.092455	69.528961
994.003274	4.423451	69.533966
993.152350	4.483186	69.538970
992.012283	1.884555	69.543975
991.839534	4.310532	69.548980
991.316686	16.065933	69.553985
990.690946	0.741924	69.558990
989.705278	12.741269	69.563994
989.146976	10.846403	69.568999
988.677968	-2.086737	69.574004
987.234563	13.609143	69.579009
986.857594	9.589731	69.584014
986.630757	3.726696	69.589018
986.066518	9.610019	69.594023
984.979845	7.797650	69.599028
984.242179	19.311279	69.604033
983.943451	14.205551	69.609038
983.464225	26.671508	69.614042
982.642409	11.164233	69.619047
981.944007	11.420468	69.624052
981.155580	14.567285	69.629057
980.619306	-2.105005	69.634062
979.302465	11.719465	69.639066
978.853856	14.288683	69.644071
978.471561	13.430217	69.649076
977.913826	12.601244	69.654081
977.728455	6.980760	69.659086
976.396677	23.699644	69.664090
976.002626	17.175686	69.669095
975.410967	9.041627	69.674100
974.216560	10.504269	69.679105
973.981513	-2.048217	69.684110
973.363408	4.559586	69.689114
972.741974	6.943422	69.694119
971.698862	10.370455	69.699124
970.533256	13.982554	69.704129
970.580539	1.998552	69.709134
970.131235	-4.843020	69.714138
969.659494	26.640664	69.719143
968.973723	3.533194	69.724148
968.037412	4.029133	69.729153
967.604938	19.292939	69.734158
966.326183	16.393123	69.739162
965.790986	17.337727	69.744167
965.432944	10.073211	69.749172
964.798671	18.985861	69.754177
964.078252	7.004172	69.759182
963.484571	6.958332	69.764186
962.828327	10.855221	69.769191
962.237177	11.926996	69.774196
961.054383	15.128688	69.779201
960.529477	10.401142	69.784206
959.998977	16.626020	69.789210
959.480762	13.508996	69.794215
958.613224	10.641517	69.799220
957.784001	22.037263	69.804225
957.859593	9.179882	69.809230
957.005246	17.859481	69.814234
955.591935	15.039427	69.819239
955.181263	3.508331	69.824244
954.799550	11.138196	69.829249
954.237941	9.529283	69.834254
953.333425	8.971533	69.839258
952.298464	18.815238	69.844263
951.979120	13.534607	69.849268
951.818337	20.772943	69.854273
950.940890	10.126645	69.859278
950.040456	9.598208	69.864282
949.167325	9.734029	69.869287
948.888445	6.189431	69.874292
948.201590	7.134518	69.879297
947.244494	10.295569	69.884302
946.958445	16.383781	69.889306
946.268435	14.090429	69.894311
945.892780	5.781665	69.899316
944.699886	15.232625	69.904321
944.404981	10.646672	69.909326
943.499150	7.856254	69.914330
942.762471	14.503435	69.919335
942.284791	10.630941	69.924340
941.575091	17.814706	69.929345
940.901265	-0.306925	69.934350
940.091423	14.636898	69.939354
939.373055	7.782954	69.944359
939.204668	15.440374	69.949364
938.596280	18.068139	69.954369
937.550248	-6.434288	69.959374
936.837573	4.676407	69.964378
936.231413	12.595872	69.969383
935.682752	6.932285	69.974388
934.705082	16.681724	69.979393
934.453199	8.736450	69.984398
933.852473	17.706841	69.989402
932.790408	20.641762	69.994407
932.074978	13.719543	69.999412
931.501862	16.094124	70.004417
931.374479	15.396942	70.009422
930.207662	10.243297	70.014426
929.684444	13.027814	70.019431
928.867355	5.068414	70.024436
928.371605	10.111401	70.029441
927.748129	-3.252859	70.034446
926.900747	13.694861	70.039450
926.405743	12.058009	70.044455
925.990206	12.359128	70.049460
924.897481	18.591485	70.054465
924.459701	13.058482	70.059470
923.965261	13.052049	70.064474
922.788367	10.907148	70.069479
922.323092	6.881303	70.074484
921.585755	12.845799	70.079489
921.279621	7.433769	70.084494
920.483545	19.612691	70.089498
919.521354	10.399099	70.094503
919.074805	11.381642	70.099508
918.378620	13.099323	70.104513
918.161294	12.154692	70.109518
917.137896	14.148365	70.114522
916.023146	14.317920	70.119527
915.971443	9.568693	70.124532
915.440934	10.507830	70.129537
914.455827	7.649618	70.134542
913.955676	10.173432	70.139546
913.267010	19.072670	70.144551
912.291483	15.932245	70.149556
911.339296	16.979490	70.154561
911.134468	8.854850	70.159566
910.746036	8.934047	70.164570
909.621262	15.721845	70.169575
909.158562	12.805724	70.174580
908.353694	14.319940	70.179585
908.270970	9.006392	70.184590
907.292493	10.390547	70.189594
906.189843	15.825005	70.194599
905.721598	1.559292	70.199604
905.074122	11.745023	70.204609
904.805446	12.648800	70.209614
903.900216	6.877973	70.214618
903.142798	5.735457	70.219623
902.965698	16.158557	70.224628
901.939217	16.202110	70.229633
901.247131	6.281670	70.234638
900.830564	10.113621	70.239642
899.898008	14.898137	70.244647
899.079573	11.105114	70.249652
898.282192	18.662374	70.254657
898.084631	5.734940	70.259662
897.459980	12.279149	70.264666
896.570931	10.482674	70.269671
896.149794	11.376024	70.274676
895.356358	15.452452	70.279681
894.777827	8.968915	70.284686
893.743946	21.553107	70.289690
893.011618	24.487603	70.294695
892.664815	9.136579	70.299700
892.093397	15.366401	70.304705
891.311112	8.760758	70.309710
890.162129	15.408918	70.314714
889.673368	19.960388	70.319719
889.587628	10.586820	70.324724
888.863073	15.366620	70.329729
888.388414	8.440792	70.334734
887.551088	14.845394	70.339738
886.911616	21.680539	70.344743
886.032724	2.128211	70.349748
884.706047	14.941920	70.354753
884.560327	6.268581	70.359758
884.264111	8.193839	70.364762
883.843514	10.798034	70.369767
882.999916	9.451629	70.374772
882.061904	18.981892	70.379777
881.640573	2.944175	70.384782
880.879472	13.747215	70.389786
879.741850	8.256226	70.394791
879.740806	8.923451	70.399796
878.998811	3.148732	70.404801
878.052355	19.337981	70.409806
877.335324	10.340846	70.414810
876.722507	7.745083	70.419815
876.624467	9.608838	70.424820
875.227827	17.387632	70.429825
874.887085	7.748737	70.434830
874.288940	18.763956	70.439834
873.351967	11.987403	70.444839
872.339999	8.909564	70.449844
871.355693	9.637096	70.454849
871.207343	4.971063	70.459854
870.821922	16.103805	70.464858
870.191062	17.421609	70.469863
870.411149	1.735954	70.474868
869.058311	19.830118	70.479873
868.539020	12.696939	70.484878
867.788390	6.510451	70.489882
866.928064	9.664012	70.494887
866.238306	19.958982	70.499892
865.613753	12.987632	70.504897
864.659312	1.890029	70.509902
863.848371	10.534353	70.514906
863.425466	6.850271	70.519911
863.488116	7.355976	70.524916
862.208988	10.216666	70.529921
861.606240	8.526016	70.534926
860.758657	12.193195	70.539930
860.649558	6.126943	70.544935
859.827648	15.370658	70.549940
858.923732	14.242012	70.554945
858.401219	9.580342	70.559950
858.018793	14.993219	70.564954
856.644280	10.533388	70.569959
856.252651	6.429607	70.574964
855.766443	20.883561	70.579969
855.260070	14.017978	70.584974
854.187588	13.906453	70.589978
853.438191	14.618678	70.594983
853.213354	12.243430	70.599988
852.281577	16.343466	70.604993
851.811959	13.092582	70.609998
851.278831	19.614350	70.615002
850.515473	19.272280	70.620007
849.453588	3.163073	70.625012
848.545763	6.827228	70.630017
848.025471	11.211838	70.635022
847.833130	9.015915	70.640026
847.587132	14.017585	70.645031
846.896049	12.883450	70.650036
845.732978	22.921039	70.655041
845.413173	3.902614	70.660046
844.489989	4.943690	70.665050
843.708310	-0.925619	70.670055
843.493535	0.004275	70.675060
842.169899	10.072145	70.680065
841.554075	9.805939	70.685070
840.888613	6.947340	70.690074
840.461910	6.657339	70.695079
840.491503	15.243571	70.700084
839.217861	17.530987	70.705089
838.453607	8.770035	70.710094
837.830679	19.292482	70.715098
837.386456	18.393436	70.720103
836.627543	5.262067	70.725108
835.808552	7.831915	70.730113
835.402088	11.479346	70.735118
834.346381	8.417947	70.740122
833.327314	2.956997	70.745127
833.076840	4.900208	70.750132
832.504044	17.300637	70.755137
832.277050	4.663321	70.760142
831.388387	1.696757	70.765146
830.193824	9.020795	70.770151
829.876318	5.100755	70.775156
829.381902	18.548380	70.780161
828.531019	8.997006	70.785166
827.486824	4.629690	70.790170
827.286461	5.989359	70.795175
827.076516	-2.829854	70.800180
826.027492	-1.098562	70.805185
825.587000	-10.060839	70.810190
825.122267	1.653775	70.815194
823.897877	4.860569	70.820199
823.098412	0.189382	70.825204
822.439184	7.781431	70.830209
822.233960	2.935231	70.835214
821.316274	3.294223	70.840218
820.274846	3.461609	70.845223
819.927935	-1.555993	70.850228
819.096127	9.474344	70.855233
818.910883	0.293244	70.860238
818.419563	1.700806	70.865242
817.453132	3.103575	70.870247
816.912345	-0.791956	70.875252
816.009177	8.494661	70.880257
814.956788	-6.770812	70.885262
814.382793	-4.787140	70.890266
814.141656	-9.528274	70.895271
813.848264	-11.649760	70.900276
812.524885	-1.533043	70.905281
811.988501	0.277493	70.910286
811.453366	-4.738528	70.915290
810.865005	-0.719957	70.920295
810.113418	-11.141790	70.925300
809.360645	2.463637	70.930305
809.132381	0.454780	70.935310
808.137505	0.608454	70.940314
807.145320	-2.068819	70.945319
806.776815	-3.949699	70.950324
806.051172	3.148318	70.955329
805.695723	-1.222974	70.960334
804.912372	-0.514792	70.965338
804.166158	-2.975762	70.970343
803.880444	-0.646909	70.975348
802.712125	1.849251	70.980353
802.037386	-10.119127	70.985358
801.446869	-0.301987	70.990362
800.835078	1.009642	70.995367
800.551183	-0.641865	71.000372
799.337307	5.489975	71.005377
799.024491	-4.189608	71.010382
798.703481	-1.453029	71.015386
797.477362	1.031835	71.020391
796.899864	-7.613746	71.025396
796.323871	-0.016024	71.030401
795.739383	-7.938276	71.035406
794.628604	1.310432	71.040410
793.815938	2.089514	71.045415
793.751202	-6.910496	71.050420
792.889717	1.178935	71.055425
791.878298	5.592853	71.060430
791.430138	-0.222302	71.065434
790.762768	6.358685	71.070439
790.716116	-1.646035	71.075444
789.636926	6.714591	71.080449
788.958702	-1.109166	71.085454
788.128219	5.731168	71.090458
787.852038	-2.628081	71.095463
786.863864	2.422355	71.100468
786.065484	8.786089	71.105473
785.503863	-4.088085	71.110478
785.118999	-2.079324	71.115482
784.703670	0.416815	71.120487
783.857837	3.396212	71.125492
782.893387	2.171580	71.130497
782.736834	-1.023473	71.135502
781.429885	0.706321	71.140506
780.468520	-3.931190	71.145511
780.679315	-4.513472	71.150516
780.104540	7.515123	71.155521
779.304788	-3.733211	71.160526
778.356123	2.036307	71.165530
777.993767	0.834092	71.170535
777.323741	-0.804825	71.175540
776.301987	-0.306251	71.180545
775.905989	-3.606681	71.185550
774.487582	0.458888	71.190554
773.762275	-0.095787	71.195559
773.643161	-5.690518	71.200564
773.133392	0.466427	71.205569
772.473607	-4.308975	71.210574
772.369440	-4.156745	71.215578
771.366031	1.930560	71.220583
770.655012	-9.139511	71.225588
770.149460	5.456276	71.230593
769.084315	-1.044363	71.235598
768.192614	2.459561	71.240602
767.696457	5.302872	71.245607
767.477671	-2.319640	71.250612
765.974318	-0.249500	71.255617
765.410712	3.590106	71.260622
764.936038	-0.180325	71.265626
764.723684	-3.964134	71.270631
764.626579	-5.862984	71.275636
763.419659	-2.376683	71.280641
762.705017	-4.189834	71.285646
761.838265	6.008747	71.290650
760.524139	-0.829125	71.295655
760.443916	0.085662	71.300660
759.402527	7.077847	71.305665
759.599333	-9.386217	71.310670
759.089714	-4.612228	71.315674
758.209897	5.668855	71.320679
757.406588	-1.225110	71.325684
756.653481	0.984202	71.330689
755.884162	5.548815	71.335694
755.263673	1.839446	71.340698
754.530865	6.634780	71.345703
753.988854	-8.596797	71.350708
752.931811	2.441023	71.355713
752.267002	2.961622	71.360718
752.233976	7.656585	71.365722
751.569837	3.463753	71.370727
750.724267	-1.047108	71.375732
749.754938	1.780079	71.380737
749.604179	-6.433554	71.385742
749.024081	7.686846	71.390746
747.892597	11.862863	71.395751
747.238676	-1.608438	71.400756
746.694078	11.806176	71.405761
746.240530	3.278060	71.410766
745.048920	2.327720	71.415770
744.378216	6.901866	71.420775
744.203065	-3.835639	71.425780
743.549892	-3.603884	71.430785
742.525076	10.560516	71.435790
742.000687	2.023181	71.440794
741.135877	9.479250	71.445799
741.016506	5.554487	71.450804
740.290426	6.442798	71.455809
739.467846	1.761130	71.460814
738.981466	3.525874	71.465818
738.310967	7.833495	71.470823
737.312911	3.725369	71.475828
736.605169	8.944055	71.480833
736.603202	-8.732526	71.485838
735.193255	1.650310	71.490842
734.354563	-2.018004	71.495847
734.048450	-5.578730	71.500852
733.664908	2.053013	71.505857
733.094487	-8.257292	71.510862
732.326854	-9.746618	71.515866
731.451485	10.100749	71.520871
730.861359	3.746838	71.525876
730.027725	13.432401	71.530881
729.330975	-5.349344	71.535886
729.005950	-11.086317	71.540890
728.328351	-0.880004	71.545895
728.141191	-4.495939	71.550900
726.634999	0.072468	71.555905
726.056762	2.884702	71.560910
725.895728	-6.994063	71.565914
724.339422	-4.194830	71.570919
724.078871	-5.186174	71.575924
723.332271	3.487356	71.580929
723.354011	-6.921961	71.585934
722.248463	-3.465974	71.590938
721.370437	9.399356	71.595943
721.032086	-8.198434	71.600948
720.446727	11.609069	71.605953
719.780170	-8.423218	71.610958
719.068182	4.601744	71.615962
717.905020	-3.304038	71.620967
717.824011	2.540229	71.625972
716.894228	-3.605059	71.630977
715.951170	6.670336	71.635982
715.449042	2.811250	71.640986
714.666411	4.459172	71.645991
714.537461	-8.359290	71.650996
713.622094	16.742341	71.656001
713.000306	4.191568	71.661006
712.620840	0.803365	71.666010
711.957274	3.443115	71.671015
711.039270	-1.981831	71.676020
710.112662	-6.697381	71.681025
709.798940	-8.516007	71.686030
709.200151	2.103522	71.691034
708.227988	5.973500	71.696039
707.770525	8.511052	71.701044
706.788229	3.075843	71.706049
706.614093	-1.720098	71.711054
705.953024	3.349241	71.716058
704.970778	0.325090	71.721063
704.930046	4.374752	71.726068
703.361267	3.000383	71.731073
702.836557	1.350964	71.736078
702.586011	1.302586	71.741082
702.041172	5.482978	71.746087
701.428481	2.672786	71.751092
700.405961	1.503163	71.756097
699.736072	-2.225130	71.761102
699.448250	-7.471303	71.766106
698.049217	0.533441	71.771111
697.554010	-0.139849	71.776116
697.026500	16.059990	71.781121
696.595377	2.184238	71.786126
696.057634	1.818906	71.791130
694.933881	-1.345127	71.796135
694.980691	-0.398530	71.801140
694.010447	3.188884	71.806145
693.192727	3.908881	71.811150
692.514261	2.129412	71.816154
691.643300	-5.286740	71.821159
691.520317	-4.904440	71.826164
690.382288	-7.351866	71.831169
689.493323	-1.038340	71.836174
689.132835	2.693245	71.841178
688.703868	0.394675	71.846183
687.867554	-6.437236	71.851188
686.777298	8.830380	71.856193
686.457619	0.085432	71.861198
686.185781	-0.964032	71.866202
685.582558	2.960741	71.871207
685.090105	6.820570	71.876212
684.167624	15.859575	71.881217
683.254659	3.088685	71.886222
682.233221	2.956490	71.891226
681.660842	0.881023	71.896231
681.668379	-11.451405	71.901236
680.758407	-4.060673	71.906241
679.873939	-6.931654	71.911246
679.355400	-0.520999	71.916250
678.531603	3.375823	71.921255
678.469563	-15.786062	71.926260
677.069359	-3.209729	71.931265
676.253966	4.009836	71.936270
676.297603	-0.112758	71.941274
675.722579	3.091620	71.946279
675.274261	-11.760622	71.951284
674.279403	-2.735330	71.956289
673.674374	-8.328362	71.961294
672.784782	-2.131422	71.966298
671.871242	-0.344375	71.971303
671.543005	2.697707	71.976308
670.107191	0.264594	71.981313
669.549463	-0.494925	71.986318
669.052036	2.354912	71.991322
668.963482	3.640019	71.996327
668.511617	-7.036059	72.001332
667.135846	-0.488895	72.006337
666.480933	4.180520	72.011342
665.896608	-3.128309	72.016346
665.694948	6.727851	72.021351
665.333633	-0.525033	72.026356
664.051115	0.448755	72.031361
663.530051	-2.790738	72.036366
663.256310	1.581444	72.041370
661.991803	2.429367	72.046375
661.249412	1.544722	72.051380
660.544694	2.786030	72.056385
660.330963	0.109429	72.061390
659.537554	2.539643	72.066394
658.576497	25.891917	72.071399
658.219418	7.317863	72.076404
657.772833	10.897591	72.081409
657.067701	4.159910	72.086414
656.062055	7.535365	72.091418
655.173792	11.893453	72.096423
655.393170	5.410653	72.101428
654.059255	17.806154	72.106433
653.377792	3.601288	72.111438
652.837850	8.063172	72.116442
652.224000	12.282947	72.121447
651.816245	-4.710860	72.126452
650.679483	3.764630	72.131457
650.278693	4.590126	72.136462
649.984187	2.233882	72.141466
648.735374	9.090411	72.146471
648.161047	2.784470	72.151476
647.477191	4.583832	72.156481
647.021221	-4.694464	72.161486
646.265402	-2.372732	72.166490
645.138260	3.931432	72.171495
644.913807	2.738815	72.176500
644.453746	10.770669	72.181505
643.844003	3.893228	72.186510
643.275001	5.582841	72.191514
642.042638	19.671522	72.196519
642.114200	8.984620	72.201524
640.796153	17.266651	72.206529
640.280766	3.096842	72.211534
639.798639	6.358970	72.216538
639.000123	10.545081	72.221543
638.466050	8.666941	72.226548
637.407655	8.323040	72.231553
637.036577	12.281815	72.236558
636.779041	6.978787	72.241562
635.576281	12.063451	72.246567
635.007787	1.938938	72.251572
634.248901	7.776047	72.256577
634.293296	-2.446067	72.261582
633.226287	12.778443	72.266586
632.524317	13.778058	72.271591
632.255341	-1.306159	72.276596
631.087157	9.407218	72.281601
630.351081	-4.486169	72.286606
629.981392	6.029080	72.291610
628.929008	10.243009	72.296615
628.232909	9.779914	72.301620
627.537406	7.184772	72.306625
627.256374	-0.713220	72.311630
626.967385	10.844118	72.316634
625.240667	13.413520	72.321639
625.232246	3.065778	72.326644
624.606653	8.008066	72.331649
623.945902	11.971976	72.336654
623.075583	9.191796	72.341658
622.442997	3.782929	72.346663
622.144390	6.501767	72.351668
621.381447	13.664113	72.356673
619.939711	8.690027	72.361678
619.625627	-4.587769	72.366682
618.993275	22.963442	72.371687
618.624286	5.339012	72.376692
618.344957	8.450579	72.381697
617.352780	7.886414	72.386702
616.770626	8.712416	72.391706
615.907706	4.656936	72.396711
615.126260	2.920698	72.401716
614.143076	15.889532	72.406721
613.690679	2.605375	72.411726
613.485885	11.159526	72.416730
612.764871	11.580307	72.421735
612.043754	-0.164583	72.426740
611.332903	9.528256	72.431745
610.573008	7.233522	72.436750
610.102941	8.412242	72.441754
608.932377	5.761885	72.446759
608.529744	5.868621	72.451764
608.272930	16.816891	72.456769
607.382394	5.373360	72.461774
606.561416	8.131243	72.466778
605.883322	8.918913	72.471783
605.531876	5.453730	72.476788
604.690107	8.911909	72.481793
604.202493	3.421614	72.486798
603.638397	-0.835988	72.491802
602.662399	2.605724	72.496807
602.132659	4.244939	72.501812
601.223800	5.832577	72.506817
600.619054	5.244559	72.511822
600.409282	4.112683	72.516826
598.858764	11.439892	72.521831
598.671359	-3.854416	72.526836
598.103772	4.609286	72.531841
597.874521	4.644256	72.536846
596.471808	7.496371	72.541850
595.630499	2.945469	72.546855
595.338933	4.947280	72.551860
594.814378	8.637202	72.556865
594.305887	1.549694	72.561870
593.497343	4.081682	72.566874
592.736288	7.397704	72.571879
592.906739	-1.534091	72.576884
591.743387	7.305188	72.581889
591.203068	2.849844	72.586894
590.511972	-3.662973	72.591898
589.223108	12.940391	72.596903
588.664949	3.482848	72.601908
588.126545	3.541829	72.606913
587.454371	7.827673	72.611918
586.784589	2.331706	72.616922
586.093784	11.436333	72.621927
585.716808	-1.341029	72.626932
585.016225	15.192295	72.631937
583.918770	3.177785	72.636942
583.125842	3.099118	72.641946
582.521534	6.902665	72.646951
582.579845	3.922556	72.651956
581.815218	6.581588	72.656961
580.734256	6.596105	72.661966
580.399049	-1.649626	72.666970
579.853840	7.537461	72.671975
578.877927	0.018227	72.676980
578.059620	6.389917	72.681985
577.643498	-0.038967	72.686990
577.379143	-4.695948	72.691994
576.314432	8.960782	72.696999
575.364886	2.205294	72.702004
574.893139	3.650781	72.707009
574.472113	12.061186	72.712014
573.347379	-1.626777	72.717018
572.787023	8.368513	72.722023
572.823775	4.770544	72.727028
571.750412	18.031287	72.732033
570.898437	-4.631609	72.737038
570.188972	4.521718	72.742042
569.584223	9.082244	72.747047
569.788396	-0.454140	72.752052
568.560563	16.415469	72.757057
567.843702	4.748761	72.762062
566.443763	11.269867	72.767066
565.488645	6.901099	72.772071
565.585200	6.355919	72.777076
564.811245	8.505530	72.782081
564.266493	10.934011	72.787086
564.551745	6.713012	72.792090
563.357681	2.066929	72.797095
562.639927	10.283334	72.802100
561.981045	6.947550	72.807105
560.959626	2.026398	72.812110
560.253977	5.477099	72.817114
559.243940	14.139015	72.822119
559.261624	2.454654	72.827124
558.748670	4.800802	72.832129
557.798618	2.700372	72.837134
557.216572	9.917492	72.842138
556.727821	5.181141	72.847143
555.808573	6.956523	72.852148
554.869393	17.989832	72.857153
554.606412	-7.163738	72.862158
554.047854	3.922469	72.867162
553.058365	11.098839	72.872167
552.639089	-2.756672	72.877172
551.802246	3.599053	72.882177
551.154971	14.798744	72.887182
550.416052	4.655675	72.892186
549.465834	0.431209	72.897191
549.466048	5.355825	72.902196
548.988589	13.130274	72.907201
547.763708	6.096970	72.912206
547.018392	-1.717589	72.917210
546.455775	15.566436	72.922215
546.021940	-2.076015	72.927220
544.780958	14.095556	72.932225
544.251984	6.295416	72.937230
543.717036	3.854491	72.942234
543.364425	13.493433	72.947239
543.331319	-1.333453	72.952244
542.105235	8.321626	72.957249
541.467004	3.424595	72.962254
540.598621	-3.938290	72.967258
539.405113	14.311940	72.972263
539.104077	1.274923	72.977268
538.539404	3.239823	72.982273
538.446571	2.511931	72.987278
537.885675	11.080230	72.992282
536.451540	16.903509	72.997287
536.147771	-3.072949	73.002292
535.129541	3.493016	73.007297
534.209142	6.004995	73.012302
533.960418	8.600782	73.017306
533.246964	5.611153	73.022311
533.009649	-1.683529	73.027316
532.005254	12.294755	73.032321
531.382581	2.380750	73.037326
531.092062	-8.081301	73.042330
530.123392	15.860363	73.047335
529.224695	0.327729	73.052340
528.504149	14.282876	73.057345
528.017990	5.778936	73.062350
527.927555	13.751923	73.067354
526.583675	17.285382	73.072359
526.205431	-0.703372	73.077364
525.712076	12.799284	73.082369
524.823951	-0.224627	73.087374
524.268484	5.132267	73.092378
523.188570	15.353829	73.097383
523.008425	0.318565	73.102388
521.509896	9.081960	73.107393
521.078608	2.491509	73.112398
520.766706	4.750446	73.117402
520.463058	1.895804	73.122407
519.819732	2.411464	73.127412
518.746736	15.758890	73.132417
518.298701	0.059858	73.137422
517.761060	-0.608212	73.142426
516.522591	7.222816	73.147431
516.027593	2.325053	73.152436
515.714797	4.722898	73.157441
514.925635	6.942752	73.162446
514.300715	6.715923	73.167450
513.567260	9.549773	73.172455
512.940211	1.470391	73.177460
512.340107	-16.632799	73.182465
511.012978	-3.746353	73.187470
510.871592	2.594783	73.192474
510.211798	-1.434668	73.197479
509.994128	-3.935589	73.202484
508.963528	16.745487	73.207489
508.289104	0.402884	73.212494
507.839251	-8.789615	73.217498
507.025436	2.520178	73.222503
506.125426	-15.713422	73.227508
505.322132	-10.473161	73.232513
505.183793	-8.738593	73.237518
504.238995	-9.598829	73.242522
503.202952	5.844692	73.247527
502.969920	-9.087518	73.252532
502.562568	-1.346317	73.257537
501.926638	-0.817638	73.262542
501.072428	-12.016166	73.267546
499.971328	2.256630	73.272551
499.838282	-8.947982	73.277556
498.787780	2.585591	73.282561
498.088357	-12.754841	73.287566
497.397087	-4.719262	73.292570
496.941316	-2.426366	73.297575
496.897730	2.342805	73.302580
495.753782	-8.334923	73.307585
494.810206	2.604477	73.312590
494.730756	-3.572105	73.317594
493.977238	11.347042	73.322599
493.083625	-4.123302	73.327604
492.413154	-5.391498	73.332609
491.690805	-3.188590	73.337614
490.693259	-5.278271	73.342618
489.891494	0.248747	73.347623
489.741555	-6.284018	73.352628
489.168435	-4.754560	73.357633
489.027964	-0.996508	73.362638
487.976769	-0.601933	73.367642
487.050279	4.240090	73.372647
486.640535	-2.796887	73.377652
485.273775	7.703759	73.382657
484.498568	-6.019331	73.387662
484.507680	-8.420766	73.392666
483.764192	-6.148260	73.397671
483.729397	-10.997908	73.402676
482.352201	5.506021	73.407681
481.952198	2.207862	73.412686
481.555933	-3.057265	73.417690
480.620879	0.048397	73.422695
479.926591	4.170637	73.427700
479.105617	3.181878	73.432705
478.731576	-7.415081	73.437710
477.657885	6.249412	73.442714
476.989033	1.415625	73.447719
476.878298	3.245142	73.452724
475.779021	-2.187091	73.457729
474.796492	-5.911233	73.462734
474.349942	-6.388811	73.467738
473.920848	-6.216340	73.472743
473.462806	-7.750176	73.477748
472.658615	-4.548672	73.482753
472.019400	-0.059906	73.487758
471.327758	0.121280	73.492762
470.632964	0.157896	73.497767
469.775204	-5.353810	73.502772
468.958920	-2.270221	73.507777
468.514569	-3.585474	73.512782
468.413436	-10.137048	73.517786
467.429206	7.272486	73.522791
466.700744	-11.846253	73.527796
466.032118	-3.393247	73.532801
465.623675	2.476372	73.537806
464.773909	-10.172005	73.542810
464.112362	7.274425	73.547815
463.245575	-12.820441	73.552820
462.393406	4.055563	73.557825
461.475236	-8.365883	73.562830
461.327547	-8.405394	73.567834
460.891603	-2.717467	73.572839
460.377064	-4.784747	73.577844
459.485477	-2.045533	73.582849
458.909183	-1.666688	73.587854
458.504409	-1.323054	73.592858
456.723663	2.666377	73.597863
456.380013	-0.927747	73.602868
456.174734	-6.060878	73.607873
455.528025	0.051698	73.612878
454.579773	6.190245	73.617882
453.625757	5.065003	73.622887
453.672580	-13.839798	73.627892
453.058009	6.399691	73.632897
452.021065	-0.821188	73.637902
451.283743	3.465605	73.642906
450.768152	1.814791	73.647911
450.410881	-3.283086	73.652916
449.605256	1.069780	73.657921
448.617926	-0.012306	73.662926
448.036885	-4.683461	73.667930
447.610899	-1.703051	73.672935
447.412993	-0.745854	73.677940
446.137448	1.449018	73.682945
445.623372	-4.927956	73.687950
444.641382	-10.363089	73.692954
443.455396	3.935865	73.697959
443.236900	-5.764969	73.702964
442.720653	-1.448748	73.707969
442.347023	-6.353212	73.712974
442.238511	-0.460421	73.717978
441.143647	1.399750	73.722983
440.581186	-10.441299	73.727988
439.137309	-1.817457	73.732993
438.278260	-6.299240	73.737998
437.661598	-4.948905	73.743002
437.263612	2.445474	73.748007
437.134533	-9.745311	73.753012
436.903453	-0.363848	73.758017
436.114667	-0.469935	73.763022
435.346814	-7.659564	73.768026
434.231889	-7.328925	73.773031
433.671516	-5.050890	73.778036
432.735711	2.164267	73.783041
432.469694	1.698930	73.788046
431.833127	-11.076437	73.793050
430.661024	-6.559524	73.798055
430.287995	-4.935785	73.803060
430.095474	-9.637301	73.808065
428.981213	-9.015043	73.813070
428.058698	-3.418309	73.818074
427.517228	-10.043213	73.823079
427.106535	-15.361216	73.828084
426.281804	3.380603	73.833089
425.542057	-0.754348	73.838094
425.609331	-19.876851	73.843098
424.597870	-5.055376	73.848103
423.683211	-10.084931	73.853108
423.323179	-7.195448	73.858113
422.412759	-14.941067	73.863118
421.487986	-7.085878	73.868122
420.415268	4.567949	73.873127
420.403822	-8.546710	73.878132
420.052631	-3.034702	73.883137
419.143343	-13.693004	73.888142
418.135247	-13.745217	73.893146
417.437590	3.361628	73.898151
417.053097	-9.597397	73.903156
416.688137	-6.599900	73.908161
416.138705	-2.320963	73.913166
415.067915	-8.295419	73.918170
414.500790	-3.051765	73.923175
413.975514	-2.121245	73.928180
412.942201	-11.917727	73.933185
412.124837	-6.668891	73.938190
412.038707	-7.569725	73.943194
411.139833	-0.683708	73.948199
410.690747	-8.073925	73.953204
409.755354	-7.393431	73.958209
409.417685	-6.324079	73.963214
408.581808	-16.077903	73.968218
407.463982	-6.088387	73.973223
407.176091	-7.802280	73.978228
406.686427	-6.621979	73.983233
406.003454	-0.595074	73.988238
405.250663	-6.951343	73.993242
404.414513	0.981192	73.998247
403.903073	-4.219836	74.003252
402.923773	-0.950985	74.008257
401.899819	-2.639047	74.013262
401.673477	-8.964090	74.018266
401.244636	1.027603	74.023271
401.124134	-13.022108	74.028276
399.688380	6.097769	74.033281
399.094632	1.311961	74.038286
398.661116	-6.219500	74.043290
398.198372	-8.851658	74.048295
397.806232	-10.137371	74.053300
396.508210	-6.399858	74.058305
396.356220	-3.505678	74.063310
395.661342	-7.671420	74.068314
394.339573	3.768223	74.073319
394.146738	-8.992688	74.078324
393.095080	-5.527810	74.083329
392.034490	-5.749835	74.088334
391.766709	-2.187528	74.093338
390.995052	4.162584	74.098343
390.852290	-8.147434	74.103348
390.634449	-3.937102	74.108353
389.515343	2.066271	74.113358
388.916223	0.565971	74.118362
388.191301	-7.253350	74.123367
387.286309	-13.009794	74.128372
386.397350	-4.893807	74.133377
386.425632	0.576656	74.138382
385.836787	-14.010248	74.143386
384.600644	-6.617917	74.148391
384.340028	-6.505392	74.153396
383.378352	-2.644859	74.158401
382.220393	3.243288	74.163406
381.850600	-7.215556	74.168410
380.865690	-5.046469	74.173415
381.120358	-4.131427	74.178420
380.378294	5.473388	74.183425
379.480870	12.945789	74.188430
378.878970	-2.734978	74.193434
378.037682	5.849638	74.198439
377.867835	-6.014536	74.203444
376.545362	-0.623695	74.208449
375.841132	-2.769532	74.213454
375.600982	3.281426	74.218458
374.874052	-0.152261	74.223463
374.229717	-3.193850	74.228468
373.302329	-3.176909	74.233473
372.754352	2.860029	74.238478
372.530784	-1.437583	74.243482
371.332898	6.016470	74.248487
370.692499	4.421832	74.253492
370.101566	7.874799	74.258497
369.839096	-2.697339	74.263502
368.994115	-5.659644	74.268506
368.270841	-3.502285	74.273511
367.831033	-0.114402	74.278516
366.603251	-2.676673	74.283521
365.845175	-9.300154	74.288526
365.747089	-8.037176	74.293530
365.143215	-4.632608	74.298535
364.410912	-5.991834	74.303540
363.460769	3.994635	74.308545
362.846893	1.649907	74.313550
362.739817	-4.383493	74.318554
361.584361	1.676143	74.323559
360.857392	-5.272402	74.328564
360.050683	0.313783	74.333569
359.742574	-2.604774	74.338574
359.100081	-14.478765	74.343578
357.965629	-5.740202	74.348583
357.785600	-8.288103	74.353588
356.943398	-3.040022	74.358593
355.972726	-2.475306	74.363598
355.424196	-7.798136	74.368602
354.944671	5.380633	74.373607
354.875496	-5.154498	74.378612
354.139789	2.421437	74.383617
352.844342	-2.015995	74.388622
352.264163	-6.124313	74.393626
351.654292	-2.154263	74.398631
351.409834	-4.275598	74.403636
349.940645	4.789121	74.408641
349.532307	-0.038835	74.413646
349.273398	1.282889	74.418650
348.187621	1.612075	74.423655
347.572786	-4.094408	74.428660
346.640631	-3.955278	74.433665
346.207817	-8.594834	74.438670
346.332527	-7.744237	74.443674
345.346598	1.290771	74.448679
344.642587	10.138935	74.453684
343.633240	14.070159	74.458689
343.296121	-12.506468	74.463694
342.644597	17.723741	74.468698
341.763175	-10.967472	74.473703
341.402255	21.901860	74.478708
340.387271	-7.420903	74.483713
339.558610	20.541604	74.488718
339.455882	-6.813524	74.493722
338.614023	-3.139220	74.498727
338.041057	15.138319	74.503732
337.283414	-20.189203	74.508737
336.438738	12.381908	74.513742
335.706458	-17.067886	74.518746
334.699931	8.530818	74.523751
334.341222	-1.292724	74.528756
333.751323	3.298594	74.533761
333.495029	3.166017	74.538766
332.766589	-7.470610	74.543770
331.643850	2.314726	74.548775
331.335072	-6.870247	74.553780
330.920210	15.499332	74.558785
330.079368	0.490571	74.563790
329.514006	-1.309971	74.568794
328.548583	7.600358	74.573799
327.823300	-7.778456	74.578804
327.051542	-3.173924	74.583809
326.329934	-5.654428	74.588814
325.945037	-4.060321	74.593818
325.462528	0.266311	74.598823
325.040525	-7.115585	74.603828
323.835013	1.470324	74.608833
323.300403	3.556628	74.613838
322.712778	7.236148	74.618842
321.677606	7.492628	74.623847
321.551559	-4.187713	74.628852
320.820014	5.972076	74.633857
320.289006	-4.762244	74.638862
319.455051	-9.189633	74.643866
318.703189	2.249089	74.648871
318.133013	-10.636158	74.653876
316.760370	-3.368690	74.658881
316.094307	-3.812829	74.663886
315.992274	-12.505645	74.668890
315.418722	-3.034909	74.673895
315.241994	-8.035382	74.678900
314.187476	-1.750553	74.683905
313.404260	-3.038573	74.688910
313.237008	-11.320467	74.693914
311.650368	2.895737	74.698919
311.272189	-6.853733	74.703924
310.875456	-4.480335	74.708929
310.176319	-5.199885	74.713934
309.436115	-10.116854	74.718938
308.638901	1.236062	74.723943
308.416507	6.397985	74.728948
307.508083	-3.169205	74.733953
306.456321	-4.657259	74.738958
306.078359	0.048509	74.743962
305.273264	-3.686494	74.748967
305.199017	2.115682	74.753972
304.207749	0.020349	74.758977
303.287469	-1.379857	74.763982
303.166930	-1.698063	74.768986
302.001287	-4.017903	74.773991
301.353703	-6.518082	74.778996
300.792209	-2.921568	74.784001
300.346125	-0.756335	74.789006
300.013937	-5.109160	74.794010
298.875161	1.103954	74.799015
298.037047	-2.964813	74.804020
297.859104	-1.168733	74.809025
296.545652	-3.318361	74.814030
296.038068	-2.655554	74.819034
295.300823	-5.786384	74.824039
295.431402	-15.129680	74.829044
294.015578	5.032529	74.834049
293.351988	-2.673536	74.839054
293.173288	-4.641351	74.844058
292.198276	0.749339	74.849063
291.891167	-2.213520	74.854068
290.828431	3.274728	74.859073
290.425630	2.635676	74.864078
289.967406	-1.350144	74.869082
288.675988	1.361398	74.874087
287.915992	-4.131125	74.879092
287.433250	-0.473048	74.884097
286.899458	6.745882	74.889102
286.651839	-7.622579	74.894106
285.180026	1.584508	74.899111
284.980953	-5.162738	74.904116
284.227089	-8.845977	74.909121
283.892349	1.797744	74.914126
283.275019	-10.740944	74.919130
282.119637	7.323508	74.924135
281.703229	-12.012027	74.929140
281.530414	-4.424883	74.934145
280.152246	0.721004	74.939150
279.933658	-13.341431	74.944154
279.058106	0.143303	74.949159
278.335707	-8.119481	74.954164
277.381160	-10.206463	74.959169
277.113582	-2.913282	74.964174
276.694685	-6.156349	74.969178
275.698343	4.681140	74.974183
275.096817	-5.920504	74.979188
274.192225	-4.956300	74.984193
273.898704	1.071630	74.989198
273.512643	-7.635831	74.994202
272.012612	-2.183524	74.999207
271.501570	-2.288102	75.004212
271.280856	9.029700	75.009217
270.746438	2.537748	75.014222
269.764020	2.181894	75.019226
269.197752	3.376009	75.024231
269.115262	-7.816122	75.029236
267.642548	11.659770	75.034241
266.890014	-0.035813	75.039246
266.883293	-1.829199	75.044250
265.693188	7.577413	75.049255
264.973419	-5.788575	75.054260
264.478676	-2.264193	75.059265
263.984508	-0.838731	75.064270
263.541360	3.215144	75.069274
262.367462	0.406229	75.074279
261.840780	0.692059	75.079284
261.360778	4.032752	75.084289
260.520271	2.722344	75.089294
260.228359	0.209633	75.094298
259.562332	1.372345	75.099303
258.437849	-1.247334	75.104308
257.476772	-4.287281	75.109313
256.911978	5.819132	75.114318
256.853218	4.180691	75.119322
256.293470	0.498054	75.124327
255.545613	-5.888907	75.129332
254.803275	1.500458	75.134337
254.064078	1.678247	75.139342
253.404436	-0.637078	75.144346
252.306531	-5.329858	75.149351
252.152625	-0.514728	75.154356
251.537894	1.678974	75.159361
250.612375	-5.979013	75.164366
250.051997	-8.666535	75.169370
249.250313	7.539169	75.174375
248.454011	-1.615379	75.179380
247.888786	-0.632728	75.184385
247.225062	5.741212	75.189390
246.729813	5.214672	75.194394
246.401737	-1.474160	75.199399
245.774543	-6.174167	75.204404
244.446621	2.092258	75.209409
244.122218	2.142428	75.214414
243.653772	-4.552409	75.219418
242.406653	-4.342530	75.224423
241.814951	-11.153327	75.229428
241.350407	0.841974	75.234433
240.638754	4.889772	75.239438
239.849832	-14.137212	75.244442
239.076606	-1.614911	75.249447
238.835609	-1.287890	75.254452
238.337689	-2.637134	75.259457
237.657703	-3.515827	75.264462
237.190448	-5.831856	75.269466
236.171370	-3.127435	75.274471
235.373291	0.366465	75.279476
234.283290	-7.468711	75.284481
233.936727	0.377935	75.289486
233.967965	-17.125642	75.294490
233.189176	-2.270250	75.299495
232.015727	-1.660545	75.304500
231.220236	-8.196012	75.309505
230.948193	-11.210179	75.314510
230.627573	-8.235498	75.319514
229.376179	-3.820970	75.324519
229.118413	-0.186135	75.329524
228.503194	2.909626	75.334529
227.420346	3.992147	75.339534
226.736357	-10.404496	75.344538
226.020093	1.979426	75.349543
225.771430	-4.480798	75.354548
224.402919	-0.793460	75.359553
223.868297	0.690496	75.364558
223.536208	-3.518835	75.369562
222.928642	5.231976	75.374567
222.671593	5.340795	75.379572
221.578004	4.330933	75.384577
221.231631	3.334407	75.389582
220.728047	-0.395020	75.394586
219.284693	12.284590	75.399591
219.245135	6.163170	75.404596
218.493464	5.874625	75.409601
217.471065	-5.836253	75.414606
216.723399	-8.489177	75.419610
216.086495	5.424284	75.424615
215.664833	-6.853852	75.429620
215.218847	-5.631595	75.434625
214.146770	3.880790	75.439630
213.502668	-5.696955	75.444634
212.957067	2.654488	75.449639
212.625661	-9.921872	75.454644
211.270491	-6.574108	75.459649
210.756861	-6.088507	75.464654
210.805975	-8.892110	75.469658
209.807721	-4.241976	75.474663
209.102225	9.173093	75.479668
208.346443	-0.777916	75.484673
207.765952	11.303686	75.489678
207.598955	2.845149	75.494682
206.257676	4.889778	75.499687
205.479881	2.506574	75.504692
205.153579	8.038289	75.509697
204.017441	1.658057	75.514702
203.345395	-2.377229	75.519706
202.346692	-0.648977	75.524711
202.485442	3.304250	75.529716
201.882422	6.541568	75.534721
201.500616	7.690521	75.539726
200.704837	-5.502478	75.544730
200.087206	8.822635	75.549735
199.551876	-6.908088	75.554740
198.152776	2.981277	75.559745
197.694389	-0.269671	75.564750
197.686213	-9.683879	75.569754
196.373952	7.541478	75.574759
195.354725	-0.111008	75.579764
195.161812	2.453828	75.584769
194.365211	7.770379	75.589774
193.947791	-8.370205	75.594778
193.161619	3.279005	75.599783
192.557377	7.204040	75.604788
191.950044	7.212597	75.609793
191.368144	1.873054	75.614798
190.311275	-10.135071	75.619802
189.398870	-1.367195	75.624807
189.146246	-1.719527	75.629812
188.887304	0.128895	75.634817
188.123279	5.304641	75.639822
187.417840	2.829487	75.644826
186.564690	5.414438	75.649831
185.980682	3.306259	75.654836
184.861500	4.668968	75.659841
183.942455	11.264972	75.664846
184.081277	-4.584270	75.669850
183.490085	4.209665	75.674855
183.255300	-2.262226	75.679860
182.234526	-1.271581	75.684865
181.248406	12.356963	75.689870
180.609753	-6.460580	75.694874
179.833343	6.492734	75.699879
179.572845	3.352157	75.704884
179.084609	4.874457	75.709889
178.059744	3.511475	75.714894
177.522575	-6.837055	75.719898
176.656929	-2.424084	75.724903
175.835025	4.534882	75.729908
175.153287	-1.801094	75.734913
174.412039	4.619912	75.739918
174.188464	5.764139	75.744922
173.492137	19.089455	75.749927
172.524057	-9.262991	75.754932
171.909884	-6.123234	75.759937
171.290929	11.639691	75.764942
171.411146	-7.986361	75.769946
169.906372	-9.562966	75.774951
169.201012	0.278874	75.779956
168.607356	15.363383	75.784961
168.306126	-3.440152	75.789966
167.516087	0.782580	75.794970
166.370964	12.197312	75.799975
166.031580	0.833272	75.804980
165.854711	0.043106	75.809985
164.891456	-4.814595	75.814990
163.901007	10.653283	75.819994
163.422902	11.656753	75.824999
162.977739	8.214477	75.830004
161.962900	0.452504	75.835009
161.508707	3.327071	75.840014
161.189710	13.927294	75.845018
160.107653	12.193410	75.850023
159.420554	6.733459	75.855028
158.544744	-2.763170	75.860033
158.082187	10.345102	75.865038
157.846909	-2.681795	75.870042
156.477133	-2.151131	75.875047
156.163808	-3.813629	75.880052
155.625721	-0.346970	75.885057
155.120256	-0.845055	75.890062
154.489071	4.850388	75.895066
153.507442	10.757822	75.900071
153.212461	8.341803	75.905076
152.038641	-1.690752	75.910081
151.056073	4.439171	75.915086
150.830675	1.034394	75.920090
150.476113	2.899643	75.925095
149.813853	-2.031276	75.930100
148.894860	-1.287071	75.935105
148.231465	-2.031196	75.940110
147.936643	-9.583128	75.945114
146.865207	-5.129451	75.950119
146.138254	-0.470516	75.955124
145.448434	5.675804	75.960129
144.835054	6.576275	75.965134
144.504600	-4.718220	75.970138
143.268129	11.495334	75.975143
142.849915	0.497091	75.980148
142.315854	2.859296	75.985153
141.807050	11.184387	75.990158
141.411822	-2.693747	75.995162
140.315777	3.500002	76.000167
139.745100	8.532973	76.005172
139.324061	-6.769694	76.010177
138.489077	-0.522960	76.015182
137.986642	9.229766	76.020186
137.006776	0.367873	76.025191
135.867001	-4.518435	76.030196
135.112229	3.073202	76.035201
134.829762	6.328803	76.040206
134.966094	-5.819099	76.045210
134.285404	-1.134424	76.050215
133.322258	1.565850	76.055220
132.515933	0.070273	76.060225
131.411011	5.085937	76.065230
130.803162	0.163692	76.070234
130.077143	7.227225	76.075239
129.908921	-4.134134	76.080244
129.679553	-0.240482	76.085249
128.353071	0.243872	76.090254
127.773203	-8.973516	76.095258
127.234881	12.222032	76.100263
126.638431	1.113450	76.105268
126.014403	-0.143124	76.110273
124.748157	6.169231	76.115278
124.843449	0.912525	76.120282
123.913811	2.082617	76.125287
123.114044	1.793887	76.130292
122.592975	4.247060	76.135297
122.110298	7.493589	76.140302
121.013763	-1.294499	76.145306
120.225674	10.228886	76.150311
119.718363	-0.777218	76.155316
119.452494	0.719094	76.160321
118.557434	1.144118	76.165326
117.441214	2.574190	76.170330
117.107367	13.723959	76.175335
116.423084	3.110333	76.180340
116.057202	-4.753523	76.185345
115.299484	7.473035	76.190350
114.865394	-0.214375	76.195354
114.161046	9.766085	76.200359
113.563948	5.871831	76.205364
112.410323	5.084472	76.210369
111.876817	10.478933	76.215374
111.624421	-1.045612	76.220378
110.617300	2.210436	76.225383
109.881695	9.228195	76.230388
109.132267	0.350069	76.235393
108.854855	0.944672	76.240398
107.957921	-1.823179	76.245402
106.839443	1.936306	76.250407
106.622871	-7.354779	76.255412
106.313352	-7.232850	76.260417
105.215926	-0.960025	76.265422
104.529035	2.300149	76.270426
103.980165	-3.367894	76.275431
103.682172	0.178753	76.280436
102.600875	-1.987289	76.285441
101.566777	5.404485	76.290446
101.504512	-4.325927	76.295450
100.879159	-2.165189	76.300455
100.539007	-9.648384	76.305460
99.668938	-5.135342	76.310465
98.829218	2.525041	76.315470
98.137915	-9.585483	76.320474
96.955746	-1.304392	76.325479
96.682992	-2.815662	76.330484
96.228088	1.476641	76.335489
95.560836	9.439092	76.340494
95.040406	-6.103164	76.345498
94.153920	6.143932	76.350503
93.805995	-1.814244	76.355508
92.832968	-5.798341	76.360513
91.787432	17.811881	76.365518
91.436751	-0.696753	76.370522
90.929159	1.175562	76.375527
90.065289	-1.152876	76.380532
89.288312	2.410237	76.385537
88.628970	5.807942	76.390542
88.349013	0.499121	76.395546
87.512606	0.794960	76.400551
86.951300	-1.884488	76.405556
86.306006	6.033462	76.410561
85.593480	13.900640	76.415566
84.871851	-1.273655	76.420570
83.930007	4.083432	76.425575
83.610847	1.702819	76.430580
83.190069	-1.434258	76.435585
82.142520	-0.447186	76.440590
81.702434	-1.337287	76.445594
80.862547	9.207240	76.450599
80.093684	3.014494	76.455604
79.190646	3.655261	76.460609
78.458933	9.953351	76.465614
78.455191	4.892202	76.470618
77.996002	13.318193	76.475623
77.075995	10.221310	76.480628
76.304317	3.417185	76.485633
75.718013	0.620306	76.490638
75.670441	-4.337659	76.495642
74.211339	7.592353	76.500647
73.592998	-3.131111	76.505652
73.052850	6.425794	76.510657
71.721068	4.758585	76.515662
71.547794	-0.057915	76.520666
70.862540	-5.150713	76.525671
70.825746	-3.107486	76.530676
69.692391	-3.339843	76.535681
68.675650	5.157719	76.540686
68.608405	-6.823674	76.545690
67.990789	2.269366	76.550695
67.212693	-5.781037	76.555700
66.153204	-3.697702	76.560705
65.607880	3.925199	76.565710
65.102760	-12.529338	76.570714
64.054883	3.908032	76.575719
63.456768	-5.464114	76.580724
63.116530	-2.844238	76.585729
62.742041	-3.576070	76.590734
61.956184	-8.413134	76.595738
60.858301	1.568595	76.600743
60.327101	-2.353496	76.605748
59.822907	-5.445726	76.610753
58.667194	-7.262426	76.615758
58.177856	-10.755973	76.620762
57.523075	-7.893553	76.625767
57.346735	-14.172899	76.630772
57.058251	0.907085	76.635777
55.907398	-2.096201	76.640782
55.652910	-12.738917	76.645786
54.575762	-7.084291	76.650791
53.474471	-9.032665	76.655796
52.897136	-6.846460	76.660801
52.535741	-4.048176	76.665806
52.324186	-3.613874	76.670810
51.351099	-0.899371	76.675815
50.612853	-0.426796	76.680820
50.061867	-1.314971	76.685825
49.208135	-2.635808	76.690830
48.480569	-12.189138	76.695834
47.334994	-15.708898	76.700839
47.096068	-9.391638	76.705844
46.717220	-4.677819	76.710849
45.740026	3.094386	76.715854
45.321940	0.973973	76.720858
44.482174	-4.272359	76.725863
44.198351	-1.122187	76.730868
43.207345	-10.449005	76.735873
41.987578	11.353520	76.740878
42.114781	-7.967710	76.745882
41.326090	6.408352	76.750887
40.575875	0.550100	76.755892
40.039013	0.421306	76.760897
39.247218	1.107419	76.765902
38.716874	-5.205348	76.770906
37.876758	-3.719935	76.775911
37.063535	-11.056703	76.780916
36.630925	-0.949276	76.785921
36.052802	-3.594491	76.790926
35.784038	-10.958176	76.795930
34.818608	1.208485	76.800935
34.224457	-0.462818	76.805940
33.295058	-2.362909	76.810945
32.275030	9.087104	76.815950
31.870558	-1.320390	76.820954
31.476933	4.982128	76.825959
31.058182	0.256823	76.830964
29.976199	-3.640485	76.835969
29.338472	-4.309826	76.840974
29.058713	-6.040733	76.845978
27.688725	0.534203	76.850983
27.285665	-4.625667	76.855988
26.489084	-6.390828	76.860993
26.207680	-3.165351	76.865998
26.148637	-0.533555	76.871002
24.851461	-2.359213	76.876007
24.331077	-6.489590	76.881012
23.146615	2.589798	76.886017
22.062989	3.737183	76.891022
21.688205	-1.280547	76.896026
21.162064	-4.033392	76.901031
20.930430	2.353669	76.906036
20.899128	-12.495476	76.911041
19.580135	6.541267	76.916046
18.939131	-2.585915	76.921050
18.225805	-0.319667	76.926055
17.464557	-7.669449	76.931060
16.600933	-10.860447	76.936065
15.769074	21.287607	76.941070
15.694622	-15.320292	76.946074
14.712134	-6.541192	76.951079
14.079527	7.237572	76.956084
13.482401	0.399324	76.961089
12.900006	-6.663609	76.966094
12.851855	-2.116069	76.971098
11.764319	-7.188832	76.976103
11.201856	3.424990	76.981108
10.507245	-6.646070	76.986113
9.414850	4.263583	76.991118
8.829958	-5.123268	76.996122
8.320772	4.558008	77.001127
7.140115	0.728486	77.006132
6.511613	-3.930240	77.011137
6.086580	4.666914	77.016142
5.825327	-6.619658	77.021147
5.181947	5.137693	77.026151
4.426150	-2.991933	77.031156
3.548567	-8.219600	77.036161