Mon Mar 08 18:35:32 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.853896	110.707489	0.000000
-0.506760	93.244942	0.005005
-1.204575	49.916382	0.010010
-3.150134	4.481576	0.015014
-8.018855	-20.511066	0.020019
-13.298150	7.393293	0.025024
-18.005552	-7.408516	0.030029
-22.416429	-22.076257	0.035034
-26.670277	22.532376	0.040038
-30.386840	-22.717587	0.045043
-34.114491	2.987138	0.050048
-37.611885	-29.209703	0.055053
-41.134530	5.217110	0.060058
-44.825054	-11.371022	0.065062
-48.775947	-18.565184	0.070067
-52.681292	-2.569267	0.075072
-56.343822	-14.454880	0.080077
-59.807847	-15.329328	0.085082
-64.171099	-3.090565	0.090086
-67.476950	-4.084848	0.095091
-71.332818	-3.324631	0.100096
-74.995203	0.086983	0.105101
-78.752105	-15.057122	0.110106
-82.893534	12.862964	0.115110
-86.161821	-23.474951	0.120115
-90.034760	1.537121	0.125120
-93.786185	0.831566	0.130125
-97.619654	-25.032460	0.135130
-101.486059	5.311560	0.140134
-105.012553	-16.827988	0.145139
-109.369019	-5.220982	0.150144
-112.846051	-6.321925	0.155149
-116.399129	-19.598351	0.160154
-120.448935	7.424113	0.165158
-123.896602	-13.195266	0.170163
-127.719415	-8.482293	0.175168
-131.845188	-9.287324	0.180173
-135.374054	-4.509280	0.185178
-138.906694	-13.484081	0.190182
-142.795791	-9.435409	0.195187
-146.489179	-2.589053	0.200192
-150.453831	-1.413983	0.205197
-153.727157	-29.973835	0.210202
-158.070934	-9.374327	0.215206
-162.110667	-23.848710	0.220211
-165.984017	-7.055115	0.225216
-169.672822	-0.023385	0.230221
-173.102983	-12.081497	0.235226
-176.973464	-0.365851	0.240230
-180.534100	-1.975300	0.245235
-184.585945	-20.320502	0.250240
-188.081806	12.612072	0.255245
-191.257615	-21.307309	0.260250
-195.433590	-5.490343	0.265254
-199.543879	4.147450	0.270259
-203.111112	-18.387528	0.275264
-206.993361	-5.867340	0.280269
-210.585241	-6.677015	0.285274
-214.471440	-22.142425	0.290278
-218.054812	19.612540	0.295283
-222.106596	5.409805	0.300288
-225.685604	-30.195475	0.305293
-229.339113	1.896580	0.310298
-233.266561	-1.674219	0.315302
-237.126461	-16.746420	0.320307
-240.834759	-4.064718	0.325312
-244.003993	-6.767809	0.330317
-248.027055	-21.601069	0.335322
-252.316490	-1.382215	0.340326
-255.633827	-16.908387	0.345331
-259.821185	-0.301065	0.350336
-263.325144	-16.956438	0.355341
-266.554178	-29.882228	0.360346
-270.991014	-2.197018	0.365350
-274.297714	-25.762140	0.370355
-278.391643	9.423134	0.375360
-282.008484	-15.470674	0.380365
-285.929234	6.305684	0.385370
-290.002620	-9.897662	0.390374
-292.923711	-8.330718	0.395379
-297.144010	-4.888067	0.400384
-300.888139	8.360813	0.405389
-304.506179	-17.429997	0.410394
-308.994862	3.842565	0.415398
-312.039613	-22.080733	0.420403
-316.009526	0.875116	0.425408
-319.633255	-9.526120	0.430413
-323.478225	-13.909401	0.435418
-327.164333	-22.526685	0.440422
-330.689358	12.657731	0.445427
-334.715740	-18.747715	0.450432
-338.571420	-8.669409	0.455437
-342.192608	-26.854408	0.460442
-346.134419	-2.228378	0.465446
-349.708997	-20.934871	0.470451
-353.735157	-5.255109	0.475456
-357.313905	-12.427735	0.480461
-361.220681	-30.395226	0.485466
-365.034075	1.269951	0.490470
-368.221199	-13.759626	0.495475
-372.105411	-18.901339	0.500480
-376.567420	5.903984	0.505485
-379.658574	-36.613014	0.510490
-383.512788	-8.359954	0.515494
-387.648843	5.326913	0.520499
-391.275972	-7.872603	0.525504
-394.878452	-5.644845	0.530509
-398.505928	-26.572488	0.535514
-402.595660	3.310853	0.540518
-405.849601	-17.960266	0.545523
-410.402064	-25.627001	0.550528
-413.933600	-4.056119	0.555533
-417.642452	-10.979232	0.560538
-421.357680	-5.631740	0.565542
-425.061981	-11.784480	0.570547
-428.804353	-4.131999	0.575552
-432.938767	-4.179814	0.580557
-436.188133	-32.433946	0.585562
-440.156587	-7.122338	0.590566
-443.840221	-11.961666	0.595571
-447.415739	-6.761017	0.600576
-451.367691	16.088104	0.605581
-454.834263	-35.830009	0.610586
-459.175928	6.670691	0.615590
-462.700841	-23.795907	0.620595
-466.680713	-5.627195	0.625600
-470.609601	-8.265437	0.630605
-473.738513	-18.232953	0.635610
-477.702107	-9.535883	0.640614
-481.008583	2.780813	0.645619
-485.453995	-21.187139	0.650624
-488.843255	3.144285	0.655629
-492.893948	-18.105103	0.660634
-496.781220	10.348949	0.665638
-500.207589	-23.572460	0.670643
-503.862068	-10.053791	0.675648
-508.209559	-0.234129	0.680653
-511.259324	-27.252225	0.685658
-515.449002	-0.656297	0.690662
-519.237697	-9.280544	0.695667
-522.726170	-14.198220	0.700672
-526.548870	-3.976672	0.705677
-530.341651	2.646439	0.710682
-533.936852	-16.119526	0.715686
-538.081514	-12.603392	0.720691
-541.452790	0.031215	0.725696
-545.913070	-16.543483	0.730701
-549.199227	-7.900888	0.735706
-553.056530	-6.381203	0.740710
-556.403473	-21.462227	0.745715
-560.052240	7.832118	0.750720
-564.174546	-4.130601	0.755725
-567.936725	-40.957976	0.760730
-571.968376	20.291130	0.765734
-575.849976	-14.870974	0.770739
-579.274564	-36.032532	0.775744
-583.282043	11.126618	0.780749
-587.029054	-22.164708	0.785754
-590.777788	1.082606	0.790758
-594.189700	-2.021190	0.795763
-597.903619	-29.983240	0.800768
-601.855821	-3.390435	0.805773
-605.466817	-35.471894	0.810778
-609.226053	9.395872	0.815782
-613.524730	-23.657469	0.820787
-617.138793	-6.609778	0.825792
-620.626796	-11.838024	0.830797
-624.400747	-16.069733	0.835802
-628.230632	-28.213061	0.840806
-632.096826	12.390657	0.845811
-635.605427	-17.190472	0.850816
-639.475284	4.874696	0.855821
-642.870138	-35.527629	0.860826
-647.096019	19.479844	0.865830
-650.845092	-21.253822	0.870835
-654.524091	9.079889	0.875840
-658.551634	-0.161942	0.880845
-661.490210	-24.089577	0.885850
-665.846509	5.994408	0.890854
-669.355621	-32.379122	0.895859
-673.344916	0.044624	0.900864
-677.408499	-11.071025	0.905869
-681.108361	-12.673241	0.910874
-684.560021	-0.711542	0.915878
-688.298044	-21.092772	0.920883
-692.027649	4.538987	0.925888
-696.076108	-12.711452	0.930893
-699.619167	-4.477017	0.935898
-703.490971	5.173940	0.940902
-706.885194	-12.816492	0.945907
-710.775128	-0.992873	0.950912
-714.852127	1.498834	0.955917
-718.228385	0.691738	0.960922
-722.726139	-16.811684	0.965926
-726.229170	-8.293468	0.970931
-729.835218	-7.084868	0.975936
-733.427814	-11.455761	0.980941
-736.818642	-16.283065	0.985946
-741.383144	-1.208924	0.990950
-744.833411	-21.822104	0.995955
-748.715138	7.397740	1.000960
-752.376478	-15.247393	1.005965
-756.254391	0.000887	1.010970
-759.934049	-12.860049	1.015974
-763.576960	4.173537	1.020979
-766.770832	2.299790	1.025984
-771.156371	-3.254692	1.030989
-774.676645	-8.062831	1.035994
-778.970212	2.385731	1.040998
-782.643625	3.028047	1.046003
-786.339231	0.859223	1.051008
-789.763727	-28.875384	1.056013
-793.339165	-27.383016	1.061018
-797.315708	18.445326	1.066022
-801.098729	-23.832653	1.071027
-805.040392	6.106427	1.076032
-809.441415	6.513440	1.081037
-812.589486	11.401890	1.086042
-816.258205	-7.001786	1.091046
-819.857432	1.181878	1.096051
-823.602197	-22.413240	1.101056
-827.772160	2.055976	1.106061
-830.959055	-14.023125	1.111066
-834.869937	-9.802728	1.116070
-838.841336	-1.502782	1.121075
-842.925418	2.128765	1.126080
-846.413637	-16.505536	1.131085
-849.864652	-9.668507	1.136090
-853.687211	-10.359914	1.141094
-857.860968	4.294031	1.146099
-861.322761	-42.778303	1.151104
-865.440148	12.421776	1.156109
-868.982666	-26.616210	1.161114
-872.510556	12.298512	1.166118
-876.614911	-11.431419	1.171123
-880.182471	-8.388554	1.176128
-883.959122	-13.854083	1.181133
-887.444683	-3.092992	1.186138
-891.616854	-19.621570	1.191142
-895.581674	-3.952367	1.196147
-899.163158	-9.469574	1.201152
-902.627487	-8.300714	1.206157
-906.785357	-18.918341	1.211162
-910.384916	13.186412	1.216166
-913.754901	-9.911847	1.221171
-917.628935	-8.876147	1.226176
-921.675951	16.805101	1.231181
-925.291735	-13.600413	1.236186
-929.164455	-3.050161	1.241190
-933.153826	-4.441697	1.246195
-936.437293	-2.951643	1.251200
-940.693682	19.215187	1.256205
-944.038956	-29.118220	1.261210
-948.159809	18.349647	1.266214
-951.455697	-16.787072	1.271219
-955.355803	-9.815016	1.276224
-959.476510	0.224615	1.281229
-962.954656	-19.005570	1.286234
-966.526888	-0.294205	1.291238
-970.544780	0.695203	1.296243
-973.884782	-10.554521	1.301248
-978.112951	-4.862410	1.306253
-981.597922	-6.873803	1.311258
-985.624153	-18.092613	1.316262
-989.224806	-11.368650	1.321267
-992.922571	6.244842	1.326272
-997.129174	-7.586344	1.331277
-1000.545622	-10.318250	1.336282
-1004.667935	-5.336837	1.341286
-1008.321266	7.748733	1.346291
-1011.705171	-4.861049	1.351296
-1015.684179	1.515059	1.356301
-1019.026824	-24.600738	1.361306
-1023.300095	18.862742	1.366310
-1027.027103	-17.535759	1.371315
-1030.485588	-2.819325	1.376320
-1034.843209	9.543186	1.381325
-1038.183318	-26.937644	1.386330
-1041.830982	2.174185	1.391334
-1045.610158	-12.772292	1.396339
-1049.590815	-12.001579	1.401344
-1053.601659	14.005208	1.406349
-1056.857486	-4.553962	1.411354
-1060.500844	-10.357464	1.416358
-1064.350729	19.395435	1.421363
-1068.221420	-22.609363	1.426368
-1072.427575	17.852159	1.431373
-1075.679799	-1.767207	1.436378
-1079.740383	-9.883416	1.441382
-1083.135817	-0.866277	1.446387
-1086.659244	2.631856	1.451392
-1090.928759	-14.522545	1.456397
-1094.476134	18.293133	1.461402
-1098.600336	-2.022453	1.466406
-1102.342255	-12.397184	1.471411
-1105.795221	4.412532	1.476416
-1110.213388	1.766909	1.481421
-1113.414133	-3.093394	1.486426
-1116.697985	-12.096977	1.491430
-1120.711782	-5.123815	1.496435
-1124.340180	-23.460838	1.501440
-1128.713105	8.537655	1.506445
-1132.249442	-32.143872	1.511450
-1136.114068	20.854253	1.516454
-1139.793239	3.490380	1.521459
-1143.169619	-26.047880	1.526464
-1147.257049	9.851826	1.531469
-1151.021170	-10.882346	1.536474
-1154.854483	0.414110	1.541478
-1158.488014	-0.117815	1.546483
-1162.200742	-30.092624	1.551488
-1166.155366	8.638376	1.556493
-1169.449493	-30.112343	1.561498
-1174.006893	13.803608	1.566502
-1177.565034	-21.058937	1.571507
-1180.945601	9.602964	1.576512
-1185.371552	2.128833	1.581517
-1188.417172	-29.330827	1.586522
-1192.630809	16.427107	1.591526
-1196.340026	-8.798761	1.596531
-1199.756129	-9.852655	1.601536
-1203.351810	-2.515774	1.606541
-1207.099331	-15.418694	1.611546
-1211.417622	2.631828	1.616550
-1215.420785	-4.305953	1.621555
-1218.732066	-18.715161	1.626560
-1222.655244	-13.974961	1.631565
-1225.981811	-34.104080	1.636570
-1229.902541	14.683458	1.641574
-1234.042637	-19.690072	1.646579
-1237.373476	14.524469	1.651584
-1241.647204	-11.473516	1.656589
-1244.919591	-8.389035	1.661594
-1249.121246	-21.649685	1.666598
-1252.563259	-5.544817	1.671603
-1255.881216	-2.252768	1.676608
-1260.052704	4.969775	1.681613
-1263.769112	-17.224092	1.686618
-1268.085459	-5.208393	1.691622
-1271.239892	1.279014	1.696627
-1274.874356	-8.464533	1.701632
-1279.056125	-11.426760	1.706637
-1282.736115	-12.595984	1.711642
-1286.487884	8.889840	1.716646
-1290.197316	-29.955030	1.721651
-1294.071464	10.846274	1.726656
-1298.140115	-26.450977	1.731661
-1301.283369	11.642606	1.736666
-1305.169135	-3.537075	1.741670
-1309.332172	-17.533873	1.746675
-1312.749232	-16.051875	1.751680
-1316.635578	-1.864209	1.756685
-1319.946061	-10.934180	1.761690
-1323.501874	-11.344252	1.766694
-1327.653624	-2.633057	1.771699
-1331.359615	4.994466	1.776704
-1335.754937	1.784265	1.781709
-1339.310068	-7.468857	1.786714
-1342.732599	-6.156239	1.791718
-1346.393333	-20.263320	1.796723
-1350.182081	-16.334428	1.801728
-1354.592631	8.189872	1.806733
-1358.009412	-4.638007	1.811738
-1361.711558	-8.739650	1.816742
-1365.246403	-6.306804	1.821747
-1368.900767	-20.550474	1.826752
-1372.992969	9.528588	1.831757
-1376.506637	-29.349021	1.836762
-1380.660698	-2.290766	1.841766
-1384.746194	-14.563722	1.846771
-1388.233670	-0.345185	1.851776
-1391.729065	-7.972592	1.856781
-1395.211783	-18.873973	1.861786
-1399.085779	-7.324649	1.866790
-1402.999328	-7.283118	1.871795
-1406.658059	-21.702629	1.876800
-1410.548820	0.013749	1.881805
-1414.168558	-7.600024	1.886810
-1418.386947	-15.881139	1.891814
-1421.884945	6.012065	1.896819
-1425.418912	-31.529755	1.901824
-1429.535805	-4.893669	1.906829
-1432.677746	-31.709449	1.911834
-1436.846247	20.091938	1.916838
-1440.883073	13.363359	1.921843
-1444.558288	-27.758917	1.926848
-1448.389667	2.874527	1.931853
-1451.907941	14.310229	1.936858
-1455.688724	-13.174343	1.941862
-1459.497696	-0.194095	1.946867
-1463.249993	-6.176602	1.951872
-1467.184678	-11.048181	1.956877
-1470.563278	-10.242269	1.961882
-1474.345600	0.664915	1.966886
-1478.395124	-24.983686	1.971891
-1482.032954	0.279616	1.976896
-1485.855931	-9.166903	1.981901
-1489.382801	-2.488701	1.986906
-1493.025697	-16.365013	1.991910
-1497.199124	-1.322181	1.996915
-1501.141828	-8.349142	2.006912
-1502.011846	-26.556137	2.016909
-1499.451491	-6.712395	2.026906
-1496.462297	-17.142550	2.036902
-1494.496649	-8.170353	2.046899
-1492.554291	-17.302410	2.056896
-1490.806719	-17.896359	2.066893
-1489.019434	-0.890754	2.076890
-1486.977496	-18.660930	2.086886
-1485.087385	-5.538426	2.096883
-1482.973207	-14.843245	2.106880
-1481.142742	-19.359725	2.116877
-1479.299525	-21.290488	2.126874
-1477.768006	-11.282500	2.136870
-1475.579621	-7.715664	2.146867
-1473.553648	-8.246815	2.156864
-1471.529478	-12.069606	2.166861
-1469.981069	-8.068733	2.176858
-1468.046603	-9.515178	2.186854
-1465.971804	-18.237390	2.196851
-1464.208250	-4.811986	2.206848
-1462.296082	-0.277273	2.216845
-1460.373538	-10.203465	2.226842
-1458.564027	-5.543372	2.236838
-1456.343096	-9.460809	2.246835
-1454.556170	-14.227655	2.256832
-1452.757695	-15.800726	2.266829
-1450.888336	-16.600450	2.276826
-1449.394867	-6.720548	2.286822
-1447.552905	-8.456887	2.296819
-1445.116046	-17.255997	2.306816
-1443.537903	-9.197448	2.316813
-1441.632387	-6.246834	2.326810
-1439.414100	-15.415136	2.336806
-1437.939483	3.800469	2.346803
-1436.097134	-7.983824	2.356800
-1433.947693	-11.114572	2.366797
-1431.994953	-5.364288	2.376794
-1430.269201	-8.045116	2.386790
-1428.444434	-5.166821	2.396787
-1426.848280	-13.136621	2.406784
-1424.656715	-17.870335	2.416781
-1422.612033	-13.877832	2.426778
-1420.875343	-14.703658	2.436774
-1419.377608	2.637306	2.446771
-1416.906415	-19.663417	2.456768
-1415.194310	-14.714554	2.466765
-1413.324210	-10.908817	2.476762
-1411.422725	-14.508243	2.486758
-1409.539454	-9.910443	2.496755
-1407.433535	-19.319660	2.506752
-1405.724602	-10.579425	2.516749
-1403.998740	-8.007366	2.526746
-1402.354064	-13.657670	2.536742
-1400.154916	-19.496203	2.546739
-1398.198423	-13.754387	2.556736
-1396.383990	-10.298127	2.566733
-1394.533056	-13.485258	2.576730
-1392.929009	-7.222827	2.586726
-1390.891707	-17.989924	2.596723
-1388.858367	-20.273140	2.606720
-1387.041331	-15.689981	2.616717
-1385.222891	-5.899944	2.626714
-1383.211510	-5.160850	2.636710
-1381.536686	-11.089111	2.646707
-1379.518436	-2.431521	2.656704
-1377.609183	-13.361262	2.666701
-1375.627421	-7.673991	2.676698
-1374.099682	-9.421549	2.686694
-1371.806214	-12.731604	2.696691
-1370.347406	-9.658899	2.706688
-1368.187390	-3.973313	2.716685
-1366.510000	-12.265538	2.726682
-1364.565531	-14.240840	2.736678
-1362.559012	-21.428433	2.746675
-1360.680760	-10.523799	2.756672
-1358.661283	-1.989536	2.766669
-1357.218920	-12.672432	2.776666
-1355.113545	-17.472811	2.786662
-1353.074711	-10.162109	2.796659
-1351.609031	-7.437842	2.806656
-1349.492438	-20.578002	2.816653
-1347.572396	-9.455845	2.826650
-1345.688379	-19.097902	2.836646
-1343.978658	-6.600039	2.846643
-1342.004021	-14.834041	2.856640
-1339.852192	-5.716241	2.866637
-1338.137886	-12.203396	2.876634
-1336.298389	-16.193874	2.886630
-1334.452509	-6.708168	2.896627
-1332.946156	-12.980466	2.906624
-1330.806722	-14.030152	2.916621
-1328.764635	-18.334087	2.926618
-1327.198910	-6.218931	2.936614
-1324.970092	-9.981202	2.946611
-1322.957172	-12.513713	2.956608
-1321.367590	-9.675054	2.966605
-1319.594103	-10.573007	2.976602
-1317.501645	-11.858308	2.986598
-1315.619162	-12.401090	2.996595
-1313.879853	-2.743577	3.006592
-1312.046555	-7.741943	3.016589
-1309.957681	-9.482957	3.026586
-1308.444222	-7.824149	3.036582
-1306.503675	-14.634845	3.046579
-1304.449173	-3.081027	3.056576
-1302.411180	-9.037362	3.066573
-1300.465562	-18.521886	3.076570
-1298.649913	-12.291672	3.086566
-1296.815597	-13.624057	3.096563
-1295.203571	-7.785966	3.106560
-1293.212395	-8.268760	3.116557
-1291.061389	-12.425895	3.126554
-1289.486164	-10.325403	3.136550
-1287.748947	-15.188378	3.146547
-1285.716709	-18.090246	3.156544
-1283.684929	-15.382325	3.166541
-1281.791487	-12.282809	3.176538
-1279.759294	-13.751053	3.186534
-1278.001052	-14.979676	3.196531
-1276.550224	1.866835	3.206528
-1274.197956	-14.784500	3.216525
-1272.470323	-8.450181	3.226522
-1270.679074	-2.343922	3.236518
-1268.805374	-4.315715	3.246515
-1266.897746	-22.364228	3.256512
-1265.056826	-17.170610	3.266509
-1263.017663	-9.315164	3.276506
-1261.436442	-15.757287	3.286502
-1259.795589	3.081359	3.296499
-1257.534564	-8.698764	3.306496
-1255.571409	-16.915073	3.316493
-1253.769773	-11.573059	3.326490
-1251.711783	-14.924261	3.336486
-1249.800174	-11.833939	3.346483
-1248.401571	-17.578969	3.356480
-1246.329752	-11.321811	3.366477
-1244.489700	-6.781684	3.376474
-1242.163030	-17.804962	3.386470
-1240.388714	-18.237221	3.396467
-1238.910799	-18.634681	3.406464
-1236.927272	-3.720660	3.416461
-1235.018832	-23.476038	3.426458
-1233.296291	-6.161426	3.436454
-1231.204295	-27.657662	3.446451
-1229.349020	2.842950	3.456448
-1227.221634	-18.617909	3.466445
-1225.565917	-22.826777	3.476442
-1223.583745	-0.665520	3.486438
-1222.006660	-7.383262	3.496435
-1219.975794	-9.005973	3.506432
-1218.120074	-13.005274	3.516429
-1216.123232	-8.019708	3.526426
-1214.066324	-19.738707	3.536422
-1212.755579	-15.922244	3.546419
-1210.982200	-8.210527	3.556416
-1208.625224	-8.202333	3.566413
-1206.597151	-8.913578	3.576410
-1205.016552	-18.194372	3.586406
-1203.263588	-7.383221	3.596403
-1201.168496	-7.241543	3.606400
-1199.322900	-10.083478	3.616397
-1197.323213	-7.731903	3.626394
-1195.589559	-11.326413	3.636390
-1193.728252	-34.195635	3.646387
-1191.944470	1.998798	3.656384
-1189.686789	-23.542150	3.666381
-1187.858770	-11.669367	3.676378
-1186.608119	-4.046091	3.686374
-1184.301943	-6.728032	3.696371
-1182.318333	-14.960191	3.706368
-1180.618008	-5.485793	3.716365
-1178.571993	-10.770711	3.726362
-1176.791805	-15.067355	3.736358
-1174.928456	-18.688914	3.746355
-1173.383704	-19.319646	3.756352
-1171.306725	-10.453371	3.766349
-1168.949438	-15.863865	3.776346
-1167.229849	-3.635831	3.786342
-1165.768195	-9.736680	3.796339
-1163.604314	-23.962628	3.806336
-1161.525631	-8.904293	3.816333
-1160.081429	-11.599881	3.826330
-1158.248769	-14.619705	3.836326
-1156.228875	-18.743113	3.846323
-1154.322708	-10.045274	3.856320
-1152.333655	-8.749801	3.866317
-1150.355986	-21.824954	3.876314
-1148.630784	-14.058114	3.886310
-1146.859944	-8.414255	3.896307
-1144.962751	-6.606736	3.906304
-1143.060914	-14.227392	3.916301
-1140.833237	-11.241221	3.926298
-1139.277670	-11.782087	3.936294
-1137.471195	-5.116075	3.946291
-1135.422569	-23.026016	3.956288
-1134.026979	-12.512884	3.966285
-1131.841323	-17.480644	3.976282
-1130.042362	-12.665442	3.986278
-1127.592570	-7.218595	3.996275
-1126.221166	-8.650473	4.006272
-1124.343627	-11.914283	4.016269
-1122.385012	-6.412540	4.026266
-1120.446208	-2.519653	4.036262
-1118.621919	-11.465191	4.046259
-1116.604534	-4.720800	4.056256
-1114.866586	-11.898398	4.066253
-1112.966602	-19.671883	4.076250
-1111.263546	-5.581248	4.086246
-1109.311649	-17.610198	4.096243
-1107.511085	-14.729350	4.106240
-1105.550903	-13.634472	4.116237
-1103.502304	-13.655787	4.126234
-1101.739779	-13.932905	4.136230
-1099.804691	-12.451921	4.146227
-1098.019914	-11.028994	4.156224
-1096.048052	-18.877119	4.166221
-1094.318893	-17.178465	4.176218
-1092.188392	-9.416407	4.186214
-1090.519546	-17.389737	4.196211
-1088.642554	-3.169014	4.206208
-1086.657370	-13.918074	4.216205
-1084.663331	-17.318901	4.226202
-1083.108073	-21.203727	4.236198
-1081.087284	-13.867775	4.246195
-1079.286637	-12.930507	4.256192
-1077.511319	-12.573368	4.266189
-1075.154644	-18.023146	4.276186
-1073.595152	-22.049162	4.286182
-1071.888385	-18.856456	4.296179
-1069.743929	-9.718255	4.306176
-1067.982733	-17.006900	4.316173
-1066.281562	-11.312362	4.326170
-1064.069451	-14.347019	4.336166
-1062.043417	-3.520998	4.346163
-1060.376084	-9.810993	4.356160
-1058.774805	-20.804927	4.366157
-1057.037034	-16.745631	4.376154
-1055.047160	-14.338680	4.386150
-1052.998668	-17.814504	4.396147
-1050.968058	-6.335554	4.406144
-1049.057212	-4.716445	4.416141
-1047.240616	-16.272156	4.426138
-1045.506949	-15.502561	4.436134
-1043.757780	-11.366132	4.446131
-1041.568758	-6.848490	4.456128
-1039.746376	-18.474590	4.466125
-1038.007496	-15.694342	4.476122
-1035.970544	-18.328345	4.486118
-1034.245374	-20.295146	4.496115
-1032.407355	-11.565772	4.506112
-1030.587182	-19.643786	4.516109
-1028.559312	-20.525363	4.526106
-1026.469749	-23.396708	4.536102
-1024.685422	-16.044992	4.546099
-1022.836333	-15.339626	4.556096
-1021.103831	-11.072625	4.566093
-1019.398010	-15.110959	4.576090
-1017.191342	-14.735918	4.586086
-1015.597077	-6.952761	4.596083
-1013.404374	-15.797676	4.606080
-1011.574887	-11.964579	4.616077
-1009.900905	-16.337272	4.626074
-1007.850673	-26.207763	4.636070
-1006.360558	-16.514882	4.646067
-1004.427476	-23.164686	4.656064
-1002.183606	-17.787401	4.666061
-1000.271903	-17.554639	4.676058
-998.462119	-20.158599	4.686054
-996.496530	-12.466388	4.696051
-994.718163	-14.945328	4.706048
-993.041768	-15.315954	4.716045
-991.328973	-13.488294	4.726042
-989.069624	-20.232891	4.736038
-987.145538	-11.627761	4.746035
-985.309196	-9.061993	4.756032
-983.522879	-16.027773	4.766029
-981.969885	-19.454302	4.776026
-979.956974	-20.868682	4.786022
-977.786933	-22.486599	4.796019
-975.931752	-16.545052	4.806016
-974.025318	-18.697103	4.816013
-972.276495	-24.715868	4.826010
-970.574562	-20.636565	4.836006
-968.516002	-16.538498	4.846003
-966.329388	-16.131783	4.856000
-964.780817	-19.851263	4.865997
-962.897728	-20.529642	4.875994
-961.117696	-16.270196	4.885990
-959.080718	-24.368615	4.895987
-957.106818	-16.131408	4.905984
-955.675903	-18.287934	4.915981
-953.686593	-17.459677	4.925978
-951.446862	-11.750113	4.935974
-949.710802	-18.692044	4.945971
-948.048927	-7.130351	4.955968
-946.141496	-7.711561	4.965965
-944.058959	-11.273260	4.975962
-942.251065	-12.223797	4.985958
-940.296660	-17.965955	4.995955
-938.299618	-13.842234	5.005952
-936.788391	-14.137467	5.015949
-934.587406	-6.605984	5.025946
-932.839060	-14.729289	5.035942
-931.125876	-11.024365	5.045939
-929.170428	-10.762226	5.055936
-927.238611	-5.153396	5.065933
-925.277115	-13.964430	5.075930
-923.364424	-18.331021	5.085926
-921.679382	-7.174044	5.095923
-919.759722	-14.694760	5.105920
-917.813514	-14.808484	5.115917
-916.181283	-15.037791	5.125914
-913.850469	-19.411226	5.135910
-912.097536	-15.745800	5.145907
-910.419903	-8.995844	5.155904
-908.512843	-26.453542	5.165901
-906.635209	-22.467014	5.175898
-905.013620	-17.334337	5.185894
-902.997607	-15.477723	5.195891
-900.891878	-21.365615	5.205888
-899.117144	-17.506305	5.215885
-897.203815	-10.033003	5.225882
-895.142962	-6.359949	5.235878
-893.508640	-25.176077	5.245875
-891.798382	-11.340604	5.255872
-889.602934	-8.866903	5.265869
-887.797565	-14.567828	5.275866
-885.845915	-17.295433	5.285862
-883.909750	-22.144145	5.295859
-882.470049	-13.159919	5.305856
-880.175556	-12.819314	5.315853
-878.487300	-8.091990	5.325850
-876.667035	-15.371005	5.335846
-874.724616	-25.820974	5.345843
-872.683448	-17.397083	5.355840
-871.067232	-19.327404	5.365837
-869.099499	-24.056419	5.375834
-867.030621	-13.533891	5.385830
-865.353791	-20.523136	5.395827
-863.379001	-17.499426	5.405824
-861.440810	-12.687312	5.415821
-859.701678	-12.636840	5.425818
-857.890321	-15.776187	5.435814
-855.959189	-19.673591	5.445811
-853.758339	-3.682392	5.455808
-852.537323	-19.314159	5.465805
-850.574901	-10.675560	5.475802
-848.458881	-12.515241	5.485798
-846.173869	-18.845412	5.495795
-844.735406	-12.211905	5.505792
-842.970320	-15.730668	5.515789
-840.833186	-20.065181	5.525786
-839.106121	-14.731429	5.535782
-837.178036	-5.029479	5.545779
-835.320998	-3.630528	5.555776
-833.500035	-14.686297	5.565773
-831.448537	-22.120655	5.575770
-829.712094	-16.147372	5.585766
-827.491215	-10.267306	5.595763
-826.066267	-15.801596	5.605760
-824.319013	-19.991675	5.615757
-822.156851	-20.250359	5.625754
-820.089218	-21.322842	5.635750
-818.391519	-15.026003	5.645747
-816.795470	-8.547130	5.655744
-814.611923	-15.366297	5.665741
-812.885499	-21.949771	5.675738
-810.799647	-18.643779	5.685734
-808.810797	-6.314794	5.695731
-807.264477	-9.793831	5.705728
-805.197735	-12.811335	5.715725
-803.318577	-23.450082	5.725722
-801.683417	-16.096441	5.735718
-800.027382	-7.363035	5.745715
-797.919769	-6.171465	5.755712
-795.783539	-10.423696	5.765709
-793.824454	-1.492412	5.775706
-792.159719	-10.668007	5.785702
-789.920129	-13.814171	5.795699
-788.369853	-11.943016	5.805696
-786.602888	-18.335594	5.815693
-784.602275	-18.363171	5.825690
-782.623478	-17.048374	5.835686
-780.862558	-15.381399	5.845683
-779.123093	-16.595600	5.855680
-776.952809	-19.435424	5.865677
-775.224062	-10.435739	5.875674
-773.554453	-16.853800	5.885670
-771.611000	-21.583596	5.895667
-769.698559	-11.043862	5.905664
-767.679242	-29.231484	5.915661
-765.750959	-19.392147	5.925658
-763.983436	-28.595193	5.935654
-762.212210	-18.937585	5.945651
-760.307685	-15.733615	5.955648
-758.410123	-12.932722	5.965645
-756.351896	-18.942372	5.975642
-754.554852	-14.030244	5.985638
-752.624654	-20.226262	5.995635
-750.873474	-12.943224	6.005632
-749.128082	-11.515311	6.015629
-747.371909	-19.053981	6.025626
-745.187681	-11.649097	6.035622
-743.221415	-19.737631	6.045619
-741.423851	-14.108765	6.055616
-739.733288	-22.274810	6.065613
-737.513162	-7.963332	6.075610
-735.923987	-18.843053	6.085606
-734.048874	-15.689622	6.095603
-732.063936	-6.591897	6.105600
-730.370984	-9.634865	6.115597
-728.169999	-8.843399	6.125594
-726.460369	-10.191736	6.135590
-724.801833	-6.192143	6.145587
-722.426305	-14.297118	6.155584
-720.912405	-9.829167	6.165581
-719.242728	-9.156467	6.175578
-716.988539	-9.243453	6.185574
-715.175457	-15.561252	6.195571
-713.201021	-14.545684	6.205568
-711.649373	-3.550362	6.215565
-709.496130	-11.818745	6.225562
-707.712849	-13.153576	6.235558
-705.894583	-2.680830	6.245555
-703.850963	-12.155323	6.255552
-702.021634	-14.692717	6.265549
-700.001284	-12.039284	6.275546
-698.543171	-11.869583	6.285542
-696.579946	-16.698794	6.295539
-694.715516	-11.143728	6.305536
-692.662987	-9.396969	6.315533
-690.724300	-12.360759	6.325530
-688.869425	-11.753942	6.335526
-687.156725	-20.618199	6.345523
-685.033546	-20.602120	6.355520
-683.627128	-17.637432	6.365517
-681.510518	-7.577058	6.375514
-679.467796	-10.208529	6.385510
-677.342189	-5.116737	6.395507
-675.920999	-4.843231	6.405504
-673.956755	-15.579172	6.415501
-672.109161	-14.573303	6.425498
-669.958656	-10.341235	6.435494
-668.405632	-20.185714	6.445491
-666.503979	-26.384999	6.455488
-664.641120	-14.109957	6.465485
-662.681954	-13.218217	6.475482
-660.724743	-21.546811	6.485478
-658.654571	-12.685260	6.495475
-656.971338	-16.636058	6.505472
-655.480233	-11.903906	6.515469
-653.491650	-18.687049	6.525466
-651.204580	-13.021058	6.535462
-649.412023	-28.393550	6.545459
-647.698176	-12.512211	6.555456
-645.733465	-19.626256	6.565453
-643.891475	-25.403906	6.575450
-642.098360	-15.786005	6.585446
-640.235241	-16.811449	6.595443
-638.202219	-22.082797	6.605440
-636.353718	-14.325762	6.615437
-634.614453	-18.343915	6.625434
-632.589228	-4.328009	6.635430
-630.740261	-20.390007	6.645427
-628.817860	-8.252328	6.655424
-627.123686	-3.721535	6.665421
-625.414444	-14.650379	6.675418
-622.941526	-13.395437	6.685414
-621.278237	-20.658670	6.695411
-619.657733	-13.209391	6.705408
-617.580595	-13.886919	6.715405
-616.030179	-18.814323	6.725402
-614.085962	-17.377021	6.735398
-611.994907	-8.422447	6.745395
-610.152488	-5.549465	6.755392
-608.288406	-13.440007	6.765389
-606.343177	-12.132328	6.775386
-604.487102	-13.923955	6.785382
-602.548019	-16.673010	6.795379
-600.897225	-15.610384	6.805376
-598.770268	-11.792891	6.815373
-596.680542	-20.016296	6.825370
-595.105414	-13.068149	6.835366
-593.418854	-19.564589	6.845363
-591.269300	-11.871392	6.855360
-589.698118	-15.970029	6.865357
-587.894092	-19.275368	6.875354
-585.491707	-10.367343	6.885350
-583.805592	-12.326007	6.895347
-581.962270	-15.094485	6.905344
-580.316022	-17.750959	6.915341
-578.159631	-17.634305	6.925338
-576.264750	-12.755027	6.935334
-574.362338	-10.677882	6.945331
-572.617215	-21.067708	6.955328
-570.754970	-16.780030	6.965325
-568.718900	-23.766472	6.975322
-566.997896	-13.401228	6.985318
-565.331280	-20.930209	6.995315
-563.360125	-11.413303	7.005312
-561.371778	-9.542498	7.015309
-559.528018	-16.155602	7.025306
-557.469135	-14.607100	7.035302
-555.793297	-15.117849	7.045299
-553.948370	-12.363639	7.055296
-552.009825	-18.027181	7.065293
-550.088806	-11.776852	7.075290
-548.089671	-14.925440	7.085286
-546.308759	-22.703180	7.095283
-544.526722	-18.685290	7.105280
-542.386857	-13.417236	7.115277
-540.856793	-11.825306	7.125274
-538.692751	-22.288335	7.135270
-537.199528	-14.989184	7.145267
-535.237245	-14.622024	7.155264
-533.237399	-19.719051	7.165261
-531.304416	-22.599701	7.175258
-529.358346	-24.457746	7.185254
-527.732583	-28.094553	7.195251
-525.813962	-20.103898	7.205248
-523.969233	-18.840097	7.215245
-521.924753	-19.081292	7.225242
-519.773057	-20.146417	7.235238
-517.990698	-24.622930	7.245235
-516.248854	-32.552295	7.255232
-514.371018	-22.485207	7.265229
-512.840986	-26.455648	7.275226
-510.752243	-32.285241	7.285222
-508.707638	-17.703922	7.295219
-507.052609	-17.545026	7.305216
-504.938735	-24.581738	7.315213
-503.444029	-17.704362	7.325210
-501.248903	-15.546016	7.335206
-499.206093	-22.498746	7.345203
-497.712686	-17.223722	7.355200
-495.648164	-15.363447	7.365197
-493.749337	-8.481128	7.375194
-492.160420	-29.064471	7.385190
-490.013128	-22.698657	7.395187
-488.023078	-19.228656	7.405184
-486.349087	-13.110919	7.415181
-484.260554	-31.435720	7.425178
-482.809358	-12.139801	7.435174
-480.787179	-22.895905	7.445171
-478.629137	-22.732059	7.455168
-476.781951	-18.036126	7.465165
-475.141346	-19.884820	7.475162
-473.320893	-28.486685	7.485158
-471.218597	-37.954568	7.495155
-469.218439	-16.294309	7.505152
-467.495747	-18.692926	7.515149
-465.648046	-29.226950	7.525146
-463.918621	-20.936039	7.535142
-461.798905	-24.725890	7.545139
-459.838047	-25.345242	7.555136
-458.059919	-16.024776	7.565133
-456.583857	-20.479177	7.575130
-454.343821	-22.688829	7.585126
-452.653133	-20.380417	7.595123
-450.765630	-41.911366	7.605120
-448.745561	-24.212526	7.615117
-446.844169	-9.137760	7.625114
-444.916166	-18.416758	7.635110
-443.116100	-24.872806	7.645107
-441.288435	-16.768080	7.655104
-439.408129	-14.894129	7.665101
-437.656393	-16.596340	7.675098
-435.596719	-15.720461	7.685094
-433.726839	-27.319015	7.695091
-431.655500	-15.849122	7.705088
-430.227593	-19.151130	7.715085
-428.229018	-21.063267	7.725082
-426.442045	-20.802230	7.735078
-424.088879	-12.329835	7.745075
-422.502124	-14.863026	7.755072
-420.597938	-19.354189	7.765069
-418.763423	-22.364286	7.775066
-417.075698	-22.205812	7.785062
-414.932115	-10.758485	7.795059
-413.029400	-12.849507	7.805056
-411.072774	-12.050306	7.815053
-409.418178	-12.998070	7.825050
-407.309335	-13.650481	7.835046
-405.583210	-8.963577	7.845043
-404.114896	-25.267804	7.855040
-401.979351	-12.339769	7.865037
-399.876541	-13.468033	7.875034
-398.135554	-12.768597	7.885030
-396.189615	-17.487453	7.895027
-394.298073	-13.256408	7.905024
-392.428891	-8.186561	7.915021
-390.464870	-20.567461	7.925018
-388.647677	-23.636347	7.935014
-387.081189	-20.531247	7.945011
-384.943188	-15.794830	7.955008
-383.171027	-11.783127	7.965005
-381.139598	-17.025600	7.975002
-379.134299	-13.264265	7.984998
-377.619074	-15.639171	7.994995
-375.969592	-14.310925	8.004992
-373.711767	-13.155586	8.014989
-371.715822	-8.525943	8.024986
-369.849785	-19.024946	8.034982
-368.232743	-18.638845	8.044979
-366.075230	-13.577117	8.054976
-364.394608	-19.990362	8.064973
-362.481559	-3.515322	8.074970
-360.458415	-14.093085	8.084966
-358.722828	-14.209042	8.094963
-356.726885	-12.898199	8.104960
-355.176140	-9.861612	8.114957
-352.904722	-20.169540	8.124954
-351.136092	-18.718198	8.134950
-349.431667	-14.326198	8.144947
-347.605124	-11.073118	8.154944
-345.535255	-13.648649	8.164941
-343.724003	-9.207383	8.174938
-341.820062	-17.688289	8.184934
-339.926898	-18.377260	8.194931
-337.945809	-12.505793	8.204928
-336.118118	-14.423733	8.214925
-334.391423	-16.503963	8.224922
-332.528651	-13.883472	8.234918
-330.338105	-11.380038	8.244915
-328.737680	-15.712121	8.254912
-326.738634	-13.493891	8.264909
-324.921848	-17.036332	8.274906
-323.024849	-19.483199	8.284902
-321.511290	-15.881730	8.294899
-319.349633	-20.813374	8.304896
-317.341607	-13.591507	8.314893
-315.665841	-16.588821	8.324890
-313.582738	-20.049033	8.334886
-311.835180	-14.048691	8.344883
-310.055265	-11.675471	8.354880
-307.961758	-7.465539	8.364877
-306.101018	-10.996038	8.374874
-304.055771	-13.264458	8.384870
-302.428358	-15.079355	8.394867
-300.631591	-11.066778	8.404864
-298.770711	-2.387773	8.414861
-296.686285	-20.926535	8.424858
-295.076654	-20.180796	8.434854
-293.116907	-5.449916	8.444851
-291.045421	-18.959438	8.454848
-289.204811	-12.467108	8.464845
-287.686468	-17.963912	8.474842
-285.543272	-16.138114	8.484838
-283.496207	-24.346569	8.494835
-281.805091	-16.826204	8.504832
-279.846885	-31.337585	8.514829
-278.071427	-12.958483	8.524826
-276.150287	-20.278449	8.534822
-274.285879	-13.954109	8.544819
-272.266848	-21.114440	8.554816
-270.353482	-14.073203	8.564813
-269.094014	-18.232414	8.574810
-267.044300	-15.343299	8.584807
-264.616245	-20.243209	8.594803
-262.827271	-14.663106	8.604800
-261.103818	-18.931102	8.614797
-259.450413	-16.378186	8.624794
-257.016182	-13.248865	8.634791
-255.628343	-14.236051	8.644787
-253.612959	-12.977170	8.654784
-251.867511	-8.680059	8.664781
-250.028446	-16.170059	8.674778
-247.923159	-17.292271	8.684775
-246.112549	-17.156446	8.694771
-244.201036	-15.304687	8.704768
-242.336595	-15.690588	8.714765
-240.326358	-19.813294	8.724762
-238.505148	-26.989392	8.734759
-236.540906	-26.349153	8.744755
-234.829628	-12.865360	8.754752
-233.120530	-19.354118	8.764749
-231.194593	-12.076440	8.774746
-229.133659	-16.687211	8.784743
-227.471031	-16.447232	8.794739
-225.596194	-12.590735	8.804736
-223.532722	-14.776737	8.814733
-221.518475	-18.397983	8.824730
-219.863813	-20.662419	8.834727
-218.081355	-20.220514	8.844723
-215.944432	-25.544423	8.854720
-214.219956	-23.054921	8.864717
-212.718314	-22.773453	8.874714
-210.640664	-22.817580	8.884711
-208.799034	-18.584733	8.894707
-206.735191	-18.473501	8.904704
-204.805890	-21.831713	8.914701
-202.846591	-20.289114	8.924698
-201.122529	-19.361053	8.934695
-199.333081	-20.529133	8.944691
-197.158187	-17.879399	8.954688
-195.188370	-19.826230	8.964685
-193.686366	-16.077573	8.974682
-191.827400	-21.791302	8.984679
-189.870142	-18.085292	8.994675
-188.023434	-18.642000	9.004672
-186.306269	-16.784442	9.014669
-184.201995	-22.163114	9.024666
-182.097224	-18.426955	9.034663
-180.583782	-20.731986	9.044659
-178.635582	-18.999707	9.054656
-176.414888	-22.623861	9.064653
-175.018227	-16.032176	9.074650
-172.939284	-20.802084	9.084647
-171.161360	-16.192739	9.094643
-169.314923	-13.481093	9.104640
-167.140859	-3.899879	9.114637
-165.287126	-13.383142	9.124634
-163.758064	-12.054479	9.134631
-161.654192	-16.272589	9.144627
-159.770152	-21.230852	9.154624
-158.176476	-15.823179	9.164621
-156.292302	-17.225808	9.174618
-154.157503	-17.788986	9.184615
-152.266823	-17.913752	9.194611
-150.464787	-19.945877	9.204608
-148.446580	-19.254178	9.214605
-146.868562	-13.234548	9.224602
-144.908574	-10.179435	9.234599
-142.828482	-13.504821	9.244595
-140.953142	-15.916518	9.254592
-139.274379	-11.400267	9.264589
-137.253878	-6.554869	9.274586
-135.203820	-12.068534	9.284583
-133.541014	-16.410450	9.294579
-131.768374	-15.253257	9.304576
-129.952279	-11.145738	9.314573
-127.886844	-21.366933	9.324570
-126.348637	-8.671714	9.334567
-124.115671	-12.345148	9.344563
-122.156196	-10.448838	9.354560
-120.506607	-8.018365	9.364557
-118.623720	-10.327043	9.374554
-116.676177	-14.782270	9.384551
-114.675537	-3.869173	9.394547
-112.786722	-18.715165	9.404544
-111.242883	-5.684527	9.414541
-109.309393	-7.099726	9.424538
-107.291232	-7.824247	9.434535
-105.347191	-17.770280	9.444531
-103.767411	-6.256367	9.454528
-101.680440	-11.640110	9.464525
-100.127329	-18.596510	9.474522
-97.844014	-7.000630	9.484519
-95.866925	-7.857532	9.494515
-93.850837	-23.546413	9.504512
-92.310910	-11.615626	9.514509
-90.322936	-3.046713	9.524506
-88.517333	-10.411274	9.534503
-86.767036	-7.628962	9.544499
-84.862298	-16.514014	9.554496
-82.933814	-10.978125	9.564493
-80.900112	-3.925917	9.574490
-79.206491	-12.145732	9.584487
-77.304969	-12.305326	9.594483
-75.558479	-9.669236	9.604480
-73.449575	-11.979200	9.614477
-71.943757	-6.958484	9.624474
-69.577705	-13.103537	9.634471
-67.776437	-7.323138	9.644467
-65.691039	-13.134480	9.654464
-64.336766	-17.896064	9.664461
-62.554223	-3.288262	9.674458
-60.224084	-10.041767	9.684455
-58.398854	-14.573751	9.694451
-56.764544	-16.021706	9.704448
-54.729907	-2.393549	9.714445
-52.917878	-13.834224	9.724442
-51.138152	1.595065	9.734439
-49.289245	-5.449549	9.744435
-47.227797	-10.151834	9.754432
-45.431533	-17.205410	9.764429
-43.321780	-13.921480	9.774426
-41.450795	-6.333300	9.784423
-39.694086	-12.308499	9.794419
-37.911686	-10.484921	9.804416
-36.282730	-16.946562	9.814413
-34.090604	-11.692677	9.824410
-32.097579	-3.283985	9.834407
-30.310922	-15.124794	9.844403
-28.169965	-8.370690	9.854400
-26.793660	-7.833858	9.864397
-24.948367	-8.881252	9.874394
-22.926976	-12.519271	9.884391
-20.966470	-13.561355	9.894387
-19.017406	-18.111483	9.904384
-17.370527	-8.363931	9.914381
-15.369500	-11.690813	9.924378
-13.238043	-6.144607	9.934375
-11.466282	-20.834501	9.944371
-9.670353	-6.974026	9.954368
-8.095464	-9.632955	9.964365
-5.990726	-11.351692	9.974362
-4.579652	1.992306	9.984359
-3.449819	42.073967	9.994355
-2.179462	85.553226	10.004352
-0.989578	160.036243	10.014349
0.000000	226.975022	10.019354
0.375578	273.205044	10.024359
1.177125	315.969040	10.029363
1.692618	352.737640	10.034368
2.735749	382.978906	10.039373
2.370599	423.526086	10.044378
3.075300	444.886642	10.049383
3.364200	462.894779	10.054387
3.493055	472.998112	10.059392
3.812659	494.812818	10.064397
3.893997	506.946950	10.069402
4.045438	502.469591	10.074407
4.085850	510.332051	10.079411
4.156486	510.451707	10.084416
4.339475	526.910927	10.089421
4.433856	545.060576	10.094426
4.432431	547.576047	10.099431
4.619888	542.537851	10.104435
4.322741	552.460030	10.109440
4.478865	556.844270	10.114445
4.974367	557.642053	10.119450
4.606006	564.992582	10.124455
4.970475	564.250100	10.129459
4.880499	556.092819	10.134464
4.776640	554.240756	10.139469
4.911001	568.279303	10.144474
4.958736	561.363179	10.149479
5.147427	563.048825	10.154483
4.909112	583.254291	10.159488
5.289478	570.701182	10.164493
4.925183	584.164849	10.169498
5.104162	569.877692	10.174503
5.008088	586.917647	10.179507
5.250166	615.729152	10.184512
5.801337	593.557838	10.189517
5.291692	607.530406	10.194522
5.534203	603.773343	10.199527
5.673579	621.261482	10.204531
5.802662	604.019180	10.209536
5.774402	582.137417	10.214541
5.337251	604.107678	10.219546
5.768867	594.916291	10.224551
5.763070	586.871722	10.229555
5.511048	606.976906	10.234560
5.876878	613.994320	10.239565
5.903653	621.654014	10.244570
6.194567	626.800517	10.249575
5.890056	614.733492	10.254579
6.082350	625.692554	10.259584
5.841231	629.276011	10.264589
5.949138	636.754040	10.269594
6.195245	626.322783	10.274599
6.222950	631.345689	10.279603
6.049054	652.140214	10.284608
6.339514	648.156298	10.289613
6.188218	638.392384	10.294618
6.177799	637.350148	10.299623
6.477483	639.029139	10.304627
6.406729	643.481131	10.309632
6.226115	642.540155	10.314637
6.056363	653.374057	10.319642
6.488860	657.583362	10.324647
6.217493	648.078288	10.329651
6.286539	651.836207	10.334656
6.381771	656.424154	10.339661
6.677723	691.992309	10.344666
6.858874	680.555819	10.349671
6.925334	683.322259	10.354675
6.743310	710.293489	10.359680
6.900044	686.754651	10.364685
7.068545	699.395435	10.369690
7.155576	683.268341	10.374695
7.111310	683.182398	10.379699
7.073351	698.089067	10.384704
7.282911	703.756351	10.389709
7.373178	702.366892	10.394714
7.206164	700.458651	10.399719
7.133507	693.061774	10.404723
7.262029	704.903119	10.409728
7.447659	700.183704	10.414733
7.150550	713.721930	10.419738
7.629141	697.196478	10.424743
7.019612	707.835634	10.429747
6.840469	715.712723	10.434752
7.237702	702.161755	10.439757
7.209578	713.214386	10.444762
7.362111	718.135411	10.449767
7.575596	722.766020	10.454771
7.562963	727.532042	10.459776
7.788267	738.806046	10.464781
7.575980	730.616135	10.469786
7.912282	733.282777	10.474791
7.861802	738.930048	10.479795
7.881119	745.613286	10.484800
8.346073	722.749052	10.489805
7.838433	748.398761	10.494810
7.952574	739.068684	10.499815
8.149312	727.341089	10.504819
8.090117	743.736680	10.509824
8.303074	733.211286	10.514829
7.838714	746.068166	10.519834
7.786324	754.607880	10.524839
8.009010	724.432101	10.529843
8.102491	770.954711	10.534848
8.730719	754.797990	10.539853
8.917067	769.861346	10.544858
8.598236	777.025886	10.549863
8.606740	742.402519	10.554867
8.494338	779.267618	10.559872
8.481863	749.424184	10.564877
8.374114	779.239559	10.569882
8.785106	770.625364	10.574887
8.735020	770.764277	10.579891
9.006199	781.272481	10.584896
8.779244	758.479122	10.589901
8.846475	782.173243	10.594906
8.981095	778.641502	10.599911
8.799794	776.281366	10.604915
8.918294	782.442599	10.609920
9.093694	762.540279	10.614925
8.738918	787.342505	10.619930
9.099948	756.229959	10.624935
9.215585	794.962113	10.629939
9.130239	778.558052	10.634944
9.499881	756.494292	10.639949
9.191855	797.613724	10.644954
9.313955	768.862119	10.649959
9.546120	795.521442	10.654963
9.187279	774.925295	10.659968
9.546501	822.660945	10.664973
10.010280	799.129724	10.669978
9.765464	800.939733	10.674983
10.178299	774.809962	10.679987
9.576175	771.756852	10.684992
9.846651	789.470290	10.689997
9.930659	764.424314	10.695002
10.090957	796.865183	10.700007
9.940323	777.497392	10.705011
9.876780	782.068125	10.710016
10.078463	787.402383	10.715021
9.835844	774.834918	10.720026
9.665218	794.351791	10.725031
9.915889	783.153291	10.730035
10.022975	806.610860	10.735040
10.392349	819.326945	10.740045
10.268315	800.164617	10.745050
10.258688	835.974253	10.750055
9.770708	823.231413	10.755059
9.971478	815.218426	10.760064
10.450375	799.471829	10.765069
10.170395	828.781764	10.770074
10.312833	812.178908	10.775079
10.358233	829.671249	10.780083
10.088444	801.805257	10.785088
10.736379	838.046188	10.790093
10.424491	853.097632	10.795098
10.924449	820.172935	10.800103
11.054361	871.651181	10.805107
11.158801	824.240465	10.810112
11.081874	840.495490	10.815117
11.160728	817.121827	10.820122
11.075499	811.584555	10.825127
11.023430	830.685173	10.830131
10.695627	818.293684	10.835136
10.891761	811.169269	10.840141
11.128291	832.447375	10.845146
11.122803	810.430747	10.850151
11.120788	811.383590	10.855155
10.666270	835.090049	10.860160
11.091965	844.718942	10.865165
11.417368	843.045961	10.870170
11.501157	842.882823	10.875175
11.529101	845.089307	10.880179
11.581768	867.530627	10.885184
11.861410	852.951168	10.890189
11.679005	848.575834	10.895194
11.546250	848.761049	10.900199
11.956708	859.384293	10.905203
11.495573	841.556172	10.910208
11.712547	860.552417	10.915213
11.996565	836.887378	10.920218
11.685070	872.207504	10.925223
12.201842	849.412079	10.930227
11.756364	861.870230	10.935232
11.981220	865.242229	10.940237
12.245021	853.797152	10.945242
12.340696	846.672972	10.950247
12.173471	854.895168	10.955251
11.847684	821.031409	10.960256
11.920572	849.660629	10.965261
12.526941	851.919942	10.970266
12.166231	851.327800	10.975271
12.317309	868.282934	10.980275
12.383696	858.889433	10.985280
12.377890	860.677099	10.990285
12.125394	870.433099	10.995290
12.411628	864.279892	11.000295
12.351733	852.273003	11.005299
12.168894	849.782211	11.010304
12.179104	866.583191	11.015309
12.369379	864.657367	11.020314
12.266092	869.294390	11.025319
12.543520	866.663955	11.030323
12.783432	886.506561	11.035328
12.975289	885.867289	11.040333
13.057247	890.935250	11.045338
12.949890	885.779951	11.050343
13.395450	887.416783	11.055347
12.925136	866.303691	11.060352
12.963250	881.334035	11.065357
12.844268	858.195288	11.070362
13.096020	904.289381	11.075367
13.212822	871.294790	11.080371
13.214063	889.410841	11.085376
13.341258	893.451288	11.090381
13.081489	885.992690	11.095386
13.118634	884.078671	11.100391
13.387832	887.784229	11.105395
13.189078	892.217287	11.110400
13.370012	899.537147	11.115405
13.542872	874.897860	11.120410
13.530337	895.473031	11.125415
13.656631	893.514830	11.130419
13.597362	880.558481	11.135424
13.669872	890.122308	11.140429
13.546876	893.931420	11.145434
13.675952	887.759114	11.150439
13.626117	882.604104	11.155443
13.502510	914.344611	11.160448
14.328482	888.315904	11.165453
13.980409	917.671571	11.170458
14.010740	911.352575	11.175463
14.066405	921.887370	11.180467
14.288205	924.983901	11.185472
13.986500	890.223572	11.190477
14.062697	917.524591	11.195482
14.294171	905.963202	11.200487
14.423298	914.445675	11.205491
14.480212	929.225485	11.210496
14.212038	922.222378	11.215501
14.795564	896.503564	11.220506
14.433865	915.814528	11.225511
14.348518	895.723374	11.230515
14.175365	928.880049	11.235520
14.718418	901.879293	11.240525
14.573857	923.631481	11.245530
14.809524	925.360141	11.250535
14.820131	898.595701	11.255539
14.681866	921.856042	11.260544
15.051617	913.153722	11.265549
14.744536	908.631096	11.270554
14.966798	935.580842	11.275559
14.813602	917.630972	11.280563
14.764344	911.602217	11.285568
14.970325	915.344673	11.290573
14.861768	919.372265	11.295578
14.844590	912.611408	11.300583
15.318781	919.979125	11.305587
14.691068	920.061930	11.310592
14.664227	941.443704	11.315597
15.169138	923.134972	11.320602
15.268332	943.826435	11.325607
15.618899	940.868926	11.330611
15.247101	944.788697	11.335616
15.784352	948.681757	11.340621
15.795051	940.191230	11.345626
15.557078	931.617366	11.350631
15.584566	925.923299	11.355635
15.453010	919.376226	11.360640
15.638087	927.788282	11.365645
15.839510	949.488481	11.370650
15.856587	939.927748	11.375655
16.107653	930.604095	11.380659
15.637284	937.791305	11.385664
15.858233	939.727322	11.390669
15.702279	941.912688	11.395674
15.931198	944.049286	11.400679
16.185059	931.717896	11.405683
15.993083	943.061767	11.410688
16.227291	940.867149	11.415693
16.641925	947.640397	11.420698
16.073857	940.817577	11.425703
16.302391	934.943206	11.430707
16.192309	942.506623	11.435712
16.675120	935.595050	11.440717
16.631319	944.619214	11.445722
16.495494	929.807893	11.450727
16.558641	917.961100	11.455731
16.347034	924.676520	11.460736
16.591166	928.315122	11.465741
16.502129	929.770714	11.470746
16.491439	935.274518	11.475751
16.459020	943.013210	11.480755
16.318805	952.038564	11.485760
16.477975	950.603399	11.490765
16.574675	945.614232	11.495770
16.186137	945.431806	11.500775
16.700383	936.310607	11.505779
16.684330	953.623662	11.510784
16.712593	957.802911	11.515789
17.069778	971.831543	11.520794
17.362370	974.475240	11.525799
17.417642	970.877260	11.530803
17.201445	988.228585	11.535808
17.540604	976.784008	11.540813
17.292633	963.712599	11.545818
17.136307	948.045076	11.550823
17.683667	966.094623	11.555827
17.091126	971.792167	11.560832
17.400583	967.295772	11.565837
17.061028	988.643910	11.570842
17.339516	981.968332	11.575847
17.769918	969.766451	11.580851
17.652488	984.779132	11.585856
17.923880	972.897504	11.590861
17.969083	978.417642	11.595866
17.629677	974.986688	11.600871
17.876023	969.136272	11.605875
17.692293	972.893588	11.610880
17.630499	982.172963	11.615885
17.754998	973.120209	11.620890
18.039876	973.950034	11.625895
18.287532	969.799391	11.630899
17.874317	977.537332	11.635904
18.352475	967.863619	11.640909
18.163837	969.234173	11.645914
18.388281	963.426676	11.650919
18.258090	975.675364	11.655923
17.980938	978.580244	11.660928
18.119812	972.299104	11.665933
18.306730	979.155996	11.670938
18.194556	976.382672	11.675943
18.393115	965.600781	11.680947
18.102164	986.956935	11.685952
18.305515	978.735286	11.690957
18.433925	988.309187	11.695962
18.369091	986.236374	11.700967
18.728954	991.304203	11.705971
18.736222	1005.197861	11.710976
18.866944	994.084564	11.715981
18.976850	1007.143402	11.720986
18.645267	1009.041392	11.725991
19.095714	1002.075024	11.730995
18.849127	1006.542554	11.736000
19.016370	1003.928090	11.741005
19.119467	1008.890217	11.746010
19.074991	1010.343441	11.751015
19.118886	1003.115477	11.756019
19.068112	1014.112024	11.761024
19.107654	995.065277	11.766029
19.231515	1013.988265	11.771034
19.054619	1002.477737	11.776039
19.330538	1002.154643	11.781043
19.132217	1002.236773	11.786048
19.363313	992.490482	11.791053
19.315663	1015.938375	11.796058
19.123801	1009.916553	11.801063
19.459947	989.541999	11.806067
19.214366	1007.215006	11.811072
19.378151	1008.612937	11.816077
19.283959	1004.373299	11.821082
19.396552	1045.279690	11.826087
20.291285	1028.061432	11.831091
19.974976	1033.819024	11.836096
20.230587	1016.392046	11.841101
20.421310	1019.942994	11.846106
20.222490	991.316249	11.851111
20.123523	988.171802	11.856115
19.859495	1000.646865	11.861120
20.088989	1000.695458	11.866125
20.018063	998.030670	11.871130
19.845598	988.397630	11.876135
19.825840	1007.639988	11.881139
20.152681	1011.188149	11.886144
20.456863	1026.971009	11.891149
20.306773	1021.491310	11.896154
20.399085	1034.202888	11.901159
20.476313	1028.030906	11.906163
20.564145	1027.889200	11.911168
20.522494	1020.151312	11.916173
20.712068	1008.257473	11.921178
20.920146	1017.430749	11.926183
20.816213	992.346543	11.931187
20.643240	995.758368	11.936192
20.512332	982.083212	11.941197
20.817672	996.113830	11.946202
20.566704	1007.213264	11.951207
21.151972	1009.587936	11.956211
20.740465	1027.000420	11.961216
20.782104	1021.963237	11.966221
20.812207	1017.219639	11.971226
20.385834	1020.329678	11.976231
20.916899	1016.439757	11.981235
20.919283	1016.866776	11.986240
21.070038	1009.774733	11.991245
20.976129	1021.062022	11.996250
20.885640	1016.120033	12.001255
21.252095	1023.486064	12.006259
21.288787	1040.675691	12.011264
21.506608	1037.545366	12.016269
21.668118	1043.622580	12.021274
21.379980	1047.202598	12.026279
21.473494	1032.313592	12.031283
21.399729	1021.672866	12.036288
21.290302	1023.327265	12.041293
21.200503	1028.387973	12.046298
21.170304	1037.670229	12.051303
21.416347	1037.200508	12.056307
21.367321	1055.367362	12.061312
21.822712	1050.745163	12.066317
21.710555	1040.575757	12.071322
21.274146	1017.148328	12.076327
21.730774	1018.018575	12.081331
21.684135	1025.202903	12.086336
22.003235	1012.250747	12.091341
21.588887	1013.094320	12.096346
21.679210	1031.276768	12.101351
22.104141	1016.336499	12.106355
21.700414	1004.770680	12.111360
21.530198	996.636986	12.116365
21.735199	1000.654016	12.121370
21.165207	986.889608	12.126375
21.382271	992.270376	12.131379
21.319767	996.486190	12.136384
21.526278	977.345026	12.141389
21.489100	984.926801	12.146394
21.120271	990.460937	12.151399
21.628689	979.150216	12.156403
21.447012	990.837839	12.161408
21.520646	986.427935	12.166413
21.636607	992.772594	12.171418
21.397502	996.945609	12.176423
21.439359	982.985849	12.181427
21.403204	987.788825	12.186432
21.979123	990.830471	12.191437
21.653032	995.443143	12.196442
21.423530	991.204589	12.201447
21.749653	986.024275	12.206451
21.465092	996.460420	12.211456
21.438257	987.143206	12.216461
21.493326	992.448883	12.221466
21.205764	992.702945	12.226471
21.388308	995.143421	12.231475
21.579892	993.709390	12.236480
21.612631	992.336964	12.241485
21.567836	1001.638871	12.246490
21.571148	983.473142	12.251495
21.601684	974.389641	12.256499
21.429687	980.002769	12.261504
21.357687	966.688822	12.266509
21.664038	966.912817	12.271514
21.348464	971.552190	12.276519
21.517823	966.964597	12.281523
21.519064	958.073439	12.286528
21.402853	966.323831	12.291533
21.208256	969.351163	12.296538
21.069309	980.131508	12.301543
21.501121	960.902393	12.306547
21.133349	967.289496	12.311552
21.295918	975.444968	12.316557
21.493088	990.098392	12.321562
21.317259	996.607862	12.326567
21.638847	987.250849	12.331571
21.274011	984.278118	12.336576
21.644155	976.236453	12.341581
21.351136	973.708018	12.346586
21.298844	974.727238	12.351591
21.287269	972.978676	12.356595
21.504900	993.458930	12.361600
21.344281	985.516103	12.366605
21.702418	980.934668	12.371610
21.538851	984.824392	12.376615
21.151887	978.551419	12.381619
21.323395	986.666048	12.386624
21.202578	971.204151	12.391629
21.311811	996.334860	12.396634
21.666368	1004.543310	12.401639
21.667125	982.883397	12.406643
21.289415	989.596953	12.411648
21.373719	973.930448	12.416653
21.424478	968.581165	12.421658
21.358684	981.462995	12.426663
21.691640	972.067907	12.431667
21.576754	975.855246	12.436672
21.485562	973.204734	12.441677
21.507812	977.903773	12.446682
21.337205	982.639880	12.451687
21.440883	975.675212	12.456691
21.355517	982.611803	12.461696
21.496991	984.672467	12.466701
21.525586	980.985697	12.471706
21.238499	982.974359	12.476711
21.457287	972.239701	12.481715
21.638597	980.234490	12.486720
21.561840	975.354980	12.491725
21.342768	979.865423	12.496730
21.385845	976.332465	12.501735
21.517492	969.957861	12.506739
21.229833	978.951552	12.511744
21.218786	993.589301	12.516749
21.347919	983.659001	12.521754
20.911646	974.758762	12.526759
21.121922	974.465061	12.531763
21.061277	984.457048	12.536768
21.593261	1013.552701	12.541773
21.532366	1000.598081	12.546778
21.434562	1016.558584	12.551783
21.736884	1004.474875	12.556787
21.275144	1005.923682	12.561792
21.272768	982.871795	12.566797
21.490832	964.641876	12.571802
21.102245	981.697408	12.576807
21.658937	999.136795	12.581811
21.327489	993.454215	12.586816
21.329370	995.869887	12.591821
21.719294	997.141862	12.596826
21.383163	1013.285454	12.601831
21.581674	982.942678	12.606835
21.243403	981.459110	12.611840
21.322524	987.152041	12.616845
21.464080	969.445260	12.621850
21.095577	992.900134	12.626855
21.817332	991.036189	12.631859
21.492789	979.801543	12.636864
21.402425	995.538483	12.641869
21.846350	986.191921	12.646874
21.679582	985.109939	12.651879
21.721034	979.129768	12.656883
21.550210	991.558418	12.661888
21.868213	979.040136	12.666893
21.749692	999.383196	12.671898
21.632337	989.724020	12.676903
21.931640	976.076451	12.681907
21.470098	971.086421	12.686912
21.528510	957.824224	12.691917
21.330955	951.830142	12.696922
20.836773	958.242133	12.701927
21.239928	964.015841	12.706931
21.276029	978.418970	12.711936
21.392107	988.269233	12.716941
21.190978	985.234122	12.721946
21.264848	995.199932	12.726951
21.559059	978.217859	12.731955
21.351735	991.934415	12.736960
21.498010	985.494392	12.741965
21.355593	989.256162	12.746970
21.711022	993.687599	12.751975
21.557435	981.227182	12.756979
21.603691	985.155983	12.761984
21.429336	974.700070	12.766989
21.237725	974.431041	12.771994
21.239263	971.227990	12.776999
21.772934	980.582709	12.782003
20.969254	969.795077	12.787008
21.476482	987.294379	12.792013
21.736728	995.994113	12.797018
21.439704	987.259318	12.802023
21.462022	968.530749	12.807027
21.236724	964.059716	12.812032
21.135600	959.272409	12.817037
21.294776	973.794679	12.822042
21.277973	989.787967	12.827047
21.955998	990.346931	12.832051
21.444044	991.764320	12.837056
21.455359	967.611118	12.842061
21.293305	953.248663	12.847066
21.174466	961.797521	12.852071
21.476035	956.991722	12.857075
21.259122	990.149210	12.862080
21.680038	1002.160213	12.867085
21.474792	969.762395	12.872090
21.132717	964.223449	12.877095
21.488657	978.928812	12.882099
21.182906	1005.513463	12.887104
21.412196	999.735142	12.892109
21.250148	992.730843	12.897114
21.395390	1005.041286	12.902119
21.452603	997.276604	12.907123
21.462895	991.859648	12.912128
21.799960	1003.246925	12.917133
21.611912	984.074061	12.922138
21.468218	983.633384	12.927143
21.278081	962.716741	12.932147
21.385410	973.546115	12.937152
21.407230	972.758914	12.942157
21.559707	971.651249	12.947162
21.182399	965.480823	12.952167
21.256642	977.335781	12.957171
21.347367	992.452468	12.962176
21.587395	991.275645	12.967181
21.624586	983.157766	12.972186
21.679631	971.313798	12.977191
21.888909	956.575144	12.982195
21.274308	968.661383	12.987200
21.333931	975.660003	12.992205
21.789981	965.128788	12.997210
21.546443	977.244165	13.002215
21.471510	967.146146	13.007219
21.444444	972.909624	13.012224
21.587339	974.045950	13.017229
21.651187	970.960697	13.022234
21.466501	983.524017	13.027239
21.329290	980.625373	13.032243
21.380803	982.725616	13.037248
21.431185	975.490323	13.042253
21.995867	974.687506	13.047258
21.616711	977.452533	13.052263
21.361956	957.460851	13.057267
21.618307	954.876341	13.062272
21.552487	950.611693	13.067277
21.667410	943.796637	13.072282
21.198507	945.051036	13.077287
21.515692	943.592248	13.082291
21.401743	950.869277	13.087296
21.261053	954.469912	13.092301
21.308427	951.792573	13.097306
21.124546	949.633094	13.102311
21.552652	947.066925	13.107315
21.066298	950.211747	13.112320
21.184943	967.219481	13.117325
21.842174	977.185282	13.122330
21.462371	972.338336	13.127335
21.561658	958.523985	13.132339
21.058770	954.802136	13.137344
21.360162	968.677236	13.142349
21.770221	968.903615	13.147354
21.658664	963.963427	13.152359
21.636939	944.448693	13.157363
21.586342	955.175505	13.162368
21.545310	937.904742	13.167373
21.424947	938.942702	13.172378
21.363875	948.352829	13.177383
21.522447	942.921704	13.182387
21.449413	950.815113	13.187392
21.307220	951.782437	13.192397
21.258230	960.074146	13.197402
21.008144	948.968000	13.202407
21.127309	954.140437	13.207411
21.200803	956.081050	13.212416
21.208096	953.979392	13.217421
21.631428	951.281517	13.222426
21.207054	967.317705	13.227431
21.692438	972.493243	13.232435
21.743407	955.777076	13.237440
21.201730	942.077582	13.242445
21.447141	948.702777	13.247450
21.578771	954.630175	13.252455
21.361064	958.299865	13.257459
21.134809	943.003050	13.262464
21.003658	956.704270	13.267469
21.681364	952.831979	13.272474
21.136004	986.453433	13.277479
21.640399	961.597116	13.282483
21.401083	975.910126	13.287488
21.394877	974.619607	13.292493
21.648668	958.727388	13.297498
21.366253	978.189796	13.302503
21.408721	936.296983	13.307507
21.372068	981.137895	13.312512
21.222855	946.092907	13.317517
21.173900	970.289999	13.322522
20.963467	977.670740	13.327527
21.546691	964.730120	13.332531
21.273160	994.056706	13.337536
21.371378	970.812172	13.342541
21.492903	1005.554199	13.347546
21.212779	977.352040	13.352551
21.595417	999.482315	13.357555
21.477049	982.764738	13.362560
21.337103	1007.335955	13.367565
21.908833	973.756055	13.372570
21.351944	995.381720	13.377575
21.642043	996.906164	13.382579
21.549492	964.395765	13.387584
21.286615	968.987309	13.392589
21.137209	957.559165	13.397594
21.294026	983.021312	13.402599
21.780886	982.278216	13.407603
21.593450	973.227903	13.412608
21.467513	964.295522	13.417613
21.517041	970.631842	13.422618
21.129367	960.525357	13.427623
21.099153	972.286582	13.432627
21.675482	974.703675	13.437632
21.259766	982.531904	13.442637
21.412624	942.791390	13.447642
21.109441	986.354898	13.452647
21.847204	971.284356	13.457651
21.522287	988.851721	13.462656
21.099834	970.060042	13.467661
21.804553	966.998737	13.472666
21.455881	973.909507	13.477671
21.539600	962.813191	13.482675
21.215062	957.711428	13.487680
21.395170	960.160171	13.492685
21.332704	959.406914	13.497690
20.917689	975.996715	13.502695
21.154229	969.053439	13.507699
21.256192	991.695251	13.512704
21.261367	1000.169159	13.517709
21.737596	992.209916	13.522714
21.750123	983.405253	13.527719
21.945237	998.719768	13.532723
21.812948	982.225189	13.537728
21.680492	963.529195	13.542733
21.887174	962.543775	13.547738
21.611442	966.968632	13.552743
21.977231	969.207987	13.557747
21.882511	959.627224	13.562752
21.448728	937.131498	13.567757
21.776179	939.760168	13.572762
21.670223	934.926331	13.577767
21.502552	929.075728	13.582771
21.466758	928.422299	13.587776
21.100294	918.096415	13.592781
21.204729	935.765553	13.597786
21.295734	944.320358	13.602791
21.416916	925.566614	13.607795
21.535288	939.305294	13.612800
21.367867	945.351346	13.617805
21.730475	940.133690	13.622810
21.563389	926.030688	13.627815
21.454948	926.189948	13.632819
21.543653	930.864180	13.637824
21.470842	951.923715	13.642829
21.433045	921.159855	13.647834
21.147637	931.652860	13.652839
21.423758	927.347877	13.657843
21.556400	930.515400	13.662848
21.227467	930.843869	13.667853
21.477556	920.560002	13.672858
21.109485	944.587170	13.677863
21.409143	937.766308	13.682867
21.191481	943.823527	13.687872
21.430619	941.538235	13.692877
21.410829	927.684556	13.697882
21.042296	941.363697	13.702887
21.250426	936.956012	13.707891
21.273830	942.362917	13.712896
21.329616	944.126578	13.717901
21.271985	952.006492	13.722906
21.536760	963.665469	13.727911
21.722446	953.981639	13.732915
21.390170	953.236721	13.737920
21.544668	940.474886	13.742925
21.779731	932.088931	13.747930
21.152074	940.633770	13.752935
21.176527	937.084868	13.757939
21.201780	933.550033	13.762944
21.383656	938.231486	13.767949
21.444323	938.739095	13.772954
21.344073	942.446819	13.777959
21.600698	948.040461	13.782963
21.474859	940.186731	13.787968
21.586122	940.145369	13.792973
21.542258	934.532065	13.797978
21.350138	941.173420	13.802983
21.656393	924.356649	13.807987
21.807246	935.532295	13.812992
21.513285	941.797226	13.817997
21.675663	934.282314	13.823002
21.346281	947.567280	13.828007
21.557614	938.306731	13.833011
21.515954	925.670813	13.838016
21.787751	946.333176	13.843021
21.597241	937.029482	13.848026
21.510682	958.050217	13.853031
21.470932	929.016596	13.858035
21.509080	959.960266	13.863040
21.364110	925.851375	13.868045
21.407497	909.574868	13.873050
21.325150	947.537908	13.878055
21.901625	919.044702	13.883059
21.565757	943.382126	13.888064
21.676220	905.269607	13.893069
21.479320	930.199864	13.898074
21.521511	905.914105	13.903079
21.148857	911.106618	13.908083
20.955767	922.900088	13.913088
21.348237	909.262954	13.918093
21.220125	912.219745	13.923098
21.100380	925.824499	13.928103
21.235676	923.741854	13.933107
21.490710	941.566756	13.938112
21.572075	946.313128	13.943117
21.481706	935.050630	13.948122
21.428897	947.900397	13.953127
21.574046	932.116999	13.958131
21.477383	925.480778	13.963136
21.252754	923.679467	13.968141
21.450835	927.131447	13.973146
21.087380	940.483343	13.978151
21.589984	928.161171	13.983155
21.323993	941.152166	13.988160
21.401006	943.899627	13.993165
21.606539	937.289322	13.998170
21.375125	934.719529	14.003175
21.242483	928.581061	14.008179
21.370259	946.486189	14.013184
21.234457	956.184211	14.018189
21.582878	938.517526	14.023207
21.277352	954.857362	14.028224
21.368359	952.017861	14.033242
21.329270	961.395791	14.038259
21.455243	947.209718	14.043277
21.623998	946.567817	14.048295
21.396982	950.482963	14.053312
21.181855	944.955349	14.058330
21.272199	948.017673	14.063347
21.432112	955.874275	14.068365
21.303115	955.764331	14.073383
21.143697	953.991908	14.078400
21.624329	948.560958	14.083418
21.553458	952.216831	14.088435
21.259172	961.322444	14.093453
21.765000	965.471483	14.098471
21.556907	981.121011	14.103488
21.780316	989.508601	14.108506
21.819844	994.870839	14.113523
21.828112	1005.965206	14.118541
21.931119	960.454192	14.123559
21.773302	988.091062	14.128576
21.960334	957.309991	14.133594
21.728206	946.927808	14.138611
21.623605	969.853029	14.143629
22.060406	975.733893	14.148647
21.703241	976.026837	14.153664
21.771064	977.702266	14.158682
21.983310	985.860410	14.163699
22.047587	986.786106	14.168717
22.002572	973.306796	14.173735
21.947911	985.461919	14.178752
21.908099	989.814386	14.183770
21.810526	989.845715	14.188787
21.996251	995.329348	14.193805
21.899195	982.333363	14.198823
21.884604	991.328323	14.203840
22.204612	999.066610	14.208858
22.247190	987.564682	14.213875
22.225480	997.550171	14.218893
22.290575	993.563389	14.223911
22.251772	986.588831	14.228928
22.090215	989.280797	14.233946
22.379495	1005.618630	14.238963
21.912414	997.348616	14.243981
22.189904	986.243360	14.248999
22.224810	997.385380	14.254016
22.185999	997.770690	14.259034
22.305664	998.041067	14.264051
22.200305	991.501820	14.269069
22.432139	990.799522	14.274087
22.470631	991.609785	14.279104
22.436000	978.314423	14.284122
22.588390	1000.022134	14.289139
22.243923	1005.563590	14.294157
22.447410	998.830370	14.299175
22.161685	998.635314	14.304192
22.174180	992.303776	14.309210
22.106023	994.296610	14.314227
22.028186	997.486437	14.319245
22.223130	996.349594	14.324263
22.353566	996.218722	14.329280
21.979518	990.253987	14.334298
22.619564	991.863323	14.339315
22.333891	1018.526534	14.344333
22.597112	1015.573041	14.349351
22.874132	1011.305500	14.354368
22.408996	1018.453322	14.359386
22.289176	1038.722776	14.364403
22.225952	1027.118146	14.369421
22.610455	1010.608413	14.374439
22.409777	1046.859468	14.379456
22.752996	1015.759219	14.384474
22.579489	1047.574915	14.389491
22.648933	1035.774520	14.394509
22.583792	1022.175683	14.399527
22.576965	1031.652328	14.404544
22.459086	1020.817733	14.409562
22.793014	1028.284841	14.414579
22.487101	1047.654366	14.419597
23.154302	1043.634461	14.424615
23.184009	1054.082104	14.429632
23.292347	1045.802084	14.434650
23.201928	1031.318546	14.439667
22.675603	1033.216151	14.444685
23.095584	1030.300573	14.449703
22.850045	1023.091565	14.454720
22.704926	1024.141891	14.459738
23.042110	1032.799212	14.464755
22.960248	1038.412051	14.469773
23.128668	1050.526931	14.474791
22.988908	1058.149822	14.479808
23.011452	1053.737245	14.484826
23.371738	1053.107263	14.489843
22.897865	1063.693427	14.494861
23.344476	1053.492343	14.499879
23.052821	1051.258098	14.504896
23.076740	1069.250612	14.509914
23.265635	1047.894267	14.514931
23.339556	1083.189299	14.519949
23.526950	1066.556788	14.524967
23.442894	1051.004172	14.529984
23.187127	1049.495632	14.535002
23.412492	1047.575316	14.540019
23.099626	1056.661930	14.545037
23.407819	1048.021285	14.550055
23.363372	1055.721778	14.555072
23.375956	1060.276688	14.560090
23.478749	1053.049861	14.565107
23.466900	1065.237547	14.570125
23.574832	1056.347275	14.575143
23.455569	1070.873793	14.580160
23.663820	1070.395468	14.585178
23.514579	1044.627406	14.590195
23.317198	1045.267660	14.595213
23.625871	1051.818624	14.600231
23.435226	1060.619916	14.605248
23.642187	1057.198780	14.610266
23.824649	1056.609742	14.615283
23.609264	1066.162142	14.620301
23.797262	1064.532491	14.625319
23.457138	1041.446898	14.630336
23.527759	1052.355185	14.635354
23.780062	1053.702338	14.640371
23.473267	1060.936607	14.645389
23.387360	1065.331054	14.650407
23.600643	1060.902211	14.655424
23.524288	1050.823859	14.660442
23.507487	1066.840931	14.665459
23.366453	1077.617831	14.670477
23.342046	1048.831778	14.675495
23.363063	1073.670301	14.680512
23.828633	1075.154896	14.685530
24.038437	1084.570286	14.690547
24.166034	1081.396174	14.695565
24.300278	1074.272856	14.700583
24.056902	1085.825828	14.705600
24.137756	1076.329551	14.710618
24.012041	1063.896466	14.715635
23.601491	1064.249833	14.720653
24.333812	1060.757492	14.725671
24.445165	1083.420371	14.730688
24.223117	1068.778470	14.735706
24.036845	1058.708205	14.740723
23.879372	1050.310133	14.745741
24.089678	1065.086092	14.750759
23.963933	1061.269722	14.755776
24.208448	1074.418508	14.760794
24.159818	1073.762509	14.765811
24.582543	1081.391655	14.770829
24.422143	1070.079330	14.775847
24.162782	1062.993625	14.780864
23.946273	1074.246585	14.785882
24.312439	1073.283769	14.790899
24.150370	1080.419464	14.795917
24.513505	1074.253756	14.800935
24.425270	1073.602501	14.805952
24.493231	1084.866727	14.810970
24.672574	1076.760975	14.815987
24.614119	1082.418860	14.821005
24.373261	1069.338769	14.826023
24.489023	1088.995016	14.831040
24.504484	1083.068791	14.836058
24.749764	1065.672024	14.841075
24.668170	1089.246545	14.846093
24.588091	1055.421704	14.851111
24.691699	1049.410651	14.856128
24.344009	1068.398345	14.861146
24.788340	1044.517553	14.866163
24.559803	1056.849898	14.871181
24.691960	1060.237473	14.876199
24.721888	1055.656983	14.881216
24.459548	1066.552319	14.886234
24.644479	1059.776415	14.891251
24.963500	1071.470907	14.896269
24.690570	1065.350020	14.901287
25.007388	1070.586267	14.906304
24.866962	1073.092414	14.911322
24.724654	1055.184915	14.916339
24.635399	1062.203600	14.921357
24.981558	1069.514628	14.926375
25.021466	1068.180717	14.931392
24.948576	1078.566093	14.936410
25.202469	1071.387516	14.941427
24.959989	1060.761519	14.946445
25.085571	1059.418664	14.951463
24.803020	1051.954432	14.956480
25.088464	1061.870530	14.961498
25.073248	1064.463668	14.966515
25.070696	1055.218225	14.971533
25.020208	1061.049430	14.976551
25.263191	1056.930445	14.981568
25.175008	1072.118944	14.986586
24.975051	1049.720390	14.991603
24.736414	1052.865091	14.996621
24.923561	1070.896067	15.001639
25.286172	1076.546568	15.006656
25.195338	1077.385327	15.011674
25.212505	1057.852683	15.016691
24.719479	1086.428781	15.021709
25.111110	1082.396189	15.026727
25.110293	1069.296690	15.031744
25.185612	1081.657671	15.036762
25.183740	1070.156475	15.041779
25.180210	1073.413115	15.046797
25.216914	1079.383000	15.051815
25.282563	1102.721709	15.056832
25.164002	1110.059684	15.061850
25.474390	1116.468837	15.066867
25.529785	1106.364715	15.071885
25.571044	1111.555266	15.076903
25.723433	1098.984992	15.081920
25.319169	1121.643651	15.086938
25.618275	1101.064001	15.091955
25.660297	1100.201641	15.096973
25.801516	1108.228042	15.101991
25.633110	1118.841031	15.107008
25.780598	1111.246838	15.112026
25.871716	1093.547447	15.117043
25.845128	1107.249141	15.122061
25.514335	1120.223891	15.127079
26.078328	1112.190476	15.132096
25.631258	1099.294250	15.137114
25.615047	1104.621375	15.142131
25.679007	1108.479145	15.147149
25.668217	1104.367587	15.152167
26.066751	1110.696615	15.157184
25.666406	1110.272881	15.162202
25.666307	1107.104972	15.167219
25.989214	1110.466856	15.172237
25.868068	1107.025680	15.177255
25.972299	1101.297641	15.182272
25.435373	1104.544979	15.187290
25.893041	1103.319038	15.192307
25.698628	1097.007870	15.197325
25.595690	1096.593331	15.202343
26.083452	1115.894567	15.207360
26.185673	1124.232353	15.212378
26.357163	1121.906929	15.217395
26.347702	1117.005524	15.222413
26.022015	1105.098209	15.227431
26.180403	1106.704156	15.232448
26.506712	1118.381794	15.237466
26.422977	1114.585450	15.242483
26.479953	1104.534558	15.247501
26.324670	1102.610451	15.252519
26.514298	1093.619041	15.257536
26.292032	1090.324553	15.262554
26.427043	1086.940052	15.267571
26.475524	1092.211239	15.272589
26.260121	1094.435202	15.277607
26.577015	1094.664688	15.282624
26.450171	1105.978875	15.287642
26.358841	1084.300666	15.292659
26.010338	1109.412107	15.297677
26.228943	1099.374766	15.302695
26.753449	1114.437281	15.307712
26.541822	1123.185331	15.312730
26.420034	1118.267234	15.317747
26.798377	1123.355267	15.322765
26.402384	1120.008257	15.327783
26.866297	1125.243087	15.332800
26.755362	1128.372156	15.337818
26.798436	1108.772393	15.342835
26.794858	1103.528720	15.347853
26.731589	1099.335873	15.352871
26.891981	1090.559906	15.357888
26.916678	1108.599534	15.362906
26.784451	1097.457295	15.367923
26.985228	1092.391811	15.372941
26.455649	1099.196032	15.377959
26.619581	1107.096119	15.382976
26.732301	1111.771922	15.387994
26.731806	1122.675875	15.393011
26.904742	1121.831959	15.398029
27.001096	1112.120836	15.403047
27.363867	1108.967411	15.408064
27.046891	1115.695262	15.413082
26.977086	1120.179962	15.418099
27.191057	1111.043091	15.423117
27.051354	1117.349428	15.428135
26.860530	1121.516814	15.433152
27.193049	1115.217551	15.438170
27.069394	1125.371964	15.443187
27.438647	1120.968563	15.448205
27.374680	1125.180210	15.453223
27.492597	1118.309577	15.458240
26.912451	1118.458767	15.463258
27.238631	1124.212621	15.468275
27.282127	1121.117978	15.473293
27.143587	1125.660832	15.478311
27.367499	1119.830331	15.483328
27.144034	1135.493488	15.488346
27.287753	1117.692872	15.493363
27.210591	1121.079240	15.498381
27.331458	1121.984908	15.503399
27.622459	1122.264141	15.508416
27.234508	1123.870709	15.513434
27.250137	1126.262317	15.518451
27.244187	1123.389484	15.523469
26.962943	1124.958585	15.528487
27.622709	1127.340269	15.533504
27.814628	1149.167737	15.538522
27.856675	1140.921830	15.543539
27.830639	1120.722759	15.548557
27.479840	1118.694557	15.553575
27.850836	1125.122361	15.558592
27.484213	1127.475836	15.563610
27.729710	1141.596624	15.568627
28.300299	1134.605026	15.573645
27.755244	1126.888475	15.578663
27.868744	1118.138844	15.583680
27.886909	1110.565276	15.588698
27.874344	1114.040437	15.593715
27.937914	1109.918591	15.598733
27.800171	1109.580386	15.603751
27.940585	1106.585116	15.608768
28.048140	1120.312618	15.613786
27.717471	1120.845149	15.618803
28.464451	1122.116561	15.623821
27.914133	1121.148902	15.628839
27.788851	1117.849951	15.633856
27.993190	1128.206878	15.638874
28.203594	1142.844480	15.643891
28.370736	1139.763146	15.648909
28.453801	1134.268124	15.653927
27.987300	1106.718035	15.658944
27.749992	1129.883316	15.663962
27.978795	1139.910745	15.668979
28.623482	1132.083093	15.673997
27.835400	1133.797521	15.679015
27.845662	1132.075089	15.684032
28.150758	1140.388394	15.689050
28.255043	1139.479924	15.694067
28.522585	1141.018131	15.699085
28.433238	1145.723026	15.704103
28.390288	1141.355473	15.709120
27.861207	1138.824036	15.714138
27.998400	1146.832225	15.719155
28.597442	1138.365357	15.724173
28.172365	1149.687818	15.729191
28.306687	1146.125667	15.734208
28.611067	1164.098738	15.739226
28.733696	1163.560136	15.744243
29.044493	1169.362079	15.749261
28.764110	1168.398555	15.754279
28.560405	1149.218756	15.759296
28.632843	1151.255254	15.764314
29.009806	1154.768971	15.769331
29.011806	1141.074373	15.774349
28.488860	1123.122106	15.779367
28.679649	1160.133677	15.784384
28.797787	1159.053114	15.789402
29.029407	1162.365078	15.794419
29.250885	1152.879356	15.799437
28.609233	1147.020153	15.804455
28.959476	1143.261550	15.809472
29.031159	1143.992599	15.814490
28.937246	1147.041882	15.819507
29.229029	1153.488624	15.824525
28.908439	1158.338939	15.829543
29.127284	1144.271565	15.834560
29.021640	1143.053667	15.839578
28.899309	1147.526304	15.844595
29.453653	1145.561374	15.849613
29.097647	1153.863722	15.854631
29.581063	1152.831866	15.859648
29.288707	1155.311923	15.864666
29.120916	1150.291043	15.869683
29.293092	1135.910234	15.874701
29.175170	1142.274454	15.879719
29.073483	1135.061322	15.884736
29.038619	1135.586001	15.889754
29.210322	1173.352530	15.894771
29.492544	1157.551053	15.899789
29.472781	1154.787379	15.904807
29.615168	1164.724791	15.909824
29.673530	1159.924235	15.914842
29.328021	1169.464423	15.919859
29.518446	1158.047316	15.924877
29.631339	1152.670222	15.929895
29.480170	1160.425543	15.934912
29.321308	1163.917756	15.939930
29.560494	1166.788080	15.944947
29.905783	1161.968504	15.949965
29.505316	1180.080748	15.954983
29.670079	1169.584771	15.960000
29.915355	1170.575990	15.965018
29.456296	1169.703882	15.970035
29.748520	1158.339750	15.975053
29.551905	1173.724968	15.980071
29.657589	1170.697472	15.985088
29.624386	1166.256000	15.990106
29.609659	1175.457155	15.995123
29.587449	1160.482851	16.000141
29.505085	1166.850848	16.005159
29.751351	1167.566639	16.010176
30.189779	1183.268999	16.015194
29.606401	1202.992860	16.020211
30.045572	1193.077575	16.025229
30.073427	1192.863964	16.030247
29.893297	1200.414718	16.035264
30.067872	1199.545370	16.040282
30.237266	1204.076102	16.045299
30.220265	1199.576194	16.050317
29.900588	1199.366101	16.055335
30.416276	1200.872604	16.060352
30.444338	1186.874941	16.065370
30.443982	1197.568148	16.070387
30.592895	1190.270979	16.075405
30.538213	1198.780119	16.080423
30.536571	1189.378720	16.085440
30.726547	1171.298537	16.090458
30.176814	1176.776841	16.095475
30.336940	1159.838695	16.100493
30.278334	1166.945348	16.105511
30.364345	1171.683631	16.110528
30.429476	1198.262911	16.115546
30.174669	1202.626135	16.120563
30.282396	1196.504256	16.125581
30.595770	1194.733476	16.130599
30.384288	1195.906079	16.135616
30.594180	1199.079948	16.140634
30.399963	1192.461975	16.145651
30.543928	1191.437064	16.150669
30.661242	1200.179889	16.155687
30.553184	1202.617977	16.160704
30.972657	1185.816186	16.165722
30.702240	1186.888079	16.170739
30.920376	1186.145487	16.175757
31.117655	1187.613110	16.180775
30.939050	1192.851339	16.185792
31.100366	1192.479594	16.190810
31.089964	1193.901691	16.195827
30.867742	1191.752301	16.200845
30.956059	1199.120246	16.205863
31.068357	1193.420771	16.210880
31.196591	1195.415345	16.215898
30.843693	1197.776079	16.220915
31.169678	1192.819576	16.225933
31.190333	1194.944561	16.230951
31.042513	1190.275976	16.235968
30.912362	1189.450508	16.240986
30.635864	1202.185443	16.246003
30.849911	1201.514286	16.251021
31.400356	1216.491763	16.256039
31.116528	1229.311259	16.261056
31.489809	1217.597535	16.266074
31.343478	1219.244228	16.271091
31.296871	1215.519012	16.276109
31.502354	1220.477351	16.281127
31.249390	1220.821317	16.286144
31.612117	1221.424158	16.291162
31.451605	1221.290924	16.296179
31.595592	1214.112502	16.301197
31.671442	1212.205000	16.306215
31.523446	1216.373447	16.311232
31.947914	1207.928090	16.316250
31.763872	1215.279708	16.321267
31.640599	1217.501580	16.326285
31.591438	1209.073557	16.331303
31.717734	1212.779845	16.336320
31.862732	1204.070757	16.341338
31.696893	1210.782412	16.346355
31.617550	1216.245485	16.351373
31.982857	1204.369453	16.356391
31.678630	1216.256267	16.361408
31.875593	1203.510485	16.366426
31.878486	1214.178019	16.371443
31.958143	1212.625404	16.376461
32.271923	1209.022034	16.381479
31.659625	1213.769456	16.386496
31.874553	1208.091359	16.391514
31.991337	1213.965159	16.396531
31.956472	1207.142445	16.401549
32.133920	1212.945224	16.406567
31.896806	1214.987056	16.411584
32.438029	1205.981974	16.416602
31.971750	1218.484502	16.421619
32.163485	1217.333997	16.426637
32.436756	1211.429523	16.431655
32.261840	1214.749707	16.436672
32.296277	1210.687533	16.441690
32.007851	1204.753096	16.446707
32.148729	1214.531912	16.451725
32.014826	1214.491958	16.456743
31.953653	1207.118177	16.461760
32.272092	1211.150888	16.466778
32.334810	1231.591269	16.471795
32.101678	1253.315228	16.476813
32.484508	1252.854672	16.481831
32.559471	1247.393932	16.486848
32.919805	1240.607273	16.491866
32.794015	1253.989882	16.496883
32.524318	1236.821328	16.501901
32.957581	1241.996598	16.506919
32.689911	1246.248632	16.511936
32.856135	1240.892887	16.516954
33.124808	1239.508320	16.521971
33.053519	1222.968794	16.526989
32.523605	1238.816211	16.532007
32.702672	1214.000624	16.537024
33.181102	1225.440164	16.542042
32.719975	1239.928566	16.547059
32.681484	1245.948263	16.552077
33.020876	1228.032938	16.557095
32.741961	1232.178225	16.562112
33.135084	1224.695804	16.567130
33.087552	1230.943447	16.572147
33.205336	1229.180261	16.577165
33.241615	1237.022129	16.582183
33.166134	1242.755149	16.587200
33.015595	1227.507093	16.592218
33.204969	1238.508264	16.597235
33.121943	1226.283730	16.602253
33.375784	1226.554735	16.607271
32.931820	1237.079626	16.612288
33.008279	1231.802692	16.617306
33.074343	1238.600068	16.622323
32.910472	1232.532501	16.627341
33.162185	1217.657592	16.632359
32.970258	1232.054291	16.637376
33.700980	1242.085113	16.642394
33.421179	1251.245223	16.647411
33.517799	1249.708774	16.652429
33.848231	1236.800108	16.657447
33.061401	1241.466837	16.662464
33.849516	1241.688814	16.667482
33.841426	1249.404061	16.672499
33.613489	1246.110440	16.677517
33.936427	1222.512978	16.682535
33.792053	1234.660596	16.687552
34.007044	1233.792665	16.692570
33.781488	1236.686787	16.697587
33.531638	1227.406743	16.702605
33.959862	1231.648460	16.707623
33.678083	1240.130924	16.712640
33.818902	1237.755318	16.717658
33.966913	1242.853388	16.722675
34.031608	1249.276617	16.727693
33.942270	1236.817133	16.732711
34.381315	1243.035943	16.737728
34.521455	1235.567122	16.742746
34.082512	1231.132137	16.747763
33.939497	1232.647745	16.752781
34.312147	1224.352211	16.757799
33.915407	1223.325444	16.762816
34.083589	1244.395519	16.767834
34.222574	1239.901395	16.772851
34.176107	1246.984130	16.777869
34.252871	1242.470041	16.782887
34.153741	1247.296077	16.787904
34.461241	1245.867565	16.792922
34.322803	1236.774235	16.797939
33.969678	1244.365186	16.802957
34.150676	1241.119604	16.807975
34.278308	1239.131482	16.812992
34.283835	1243.358821	16.818010
34.236201	1231.391326	16.823027
34.082575	1242.860898	16.828045
34.697408	1246.023678	16.833063
34.619731	1259.982197	16.838080
34.818704	1265.015520	16.843098
34.405044	1263.906508	16.848115
34.395626	1277.308330	16.853133
35.159291	1265.603094	16.858151
34.989149	1264.134355	16.863168
34.888503	1266.357345	16.868186
34.777278	1265.016060	16.873203
34.729037	1268.662111	16.878221
35.246549	1261.310840	16.883239
34.996220	1269.896841	16.888256
35.231895	1252.386555	16.893274
35.323396	1248.812333	16.898291
34.909543	1239.423160	16.903309
34.932630	1231.740207	16.908327
35.180702	1255.452754	16.913344
35.001860	1256.141968	16.918362
35.418354	1261.019479	16.923379
35.024291	1248.586561	16.928397
35.151339	1256.056895	16.933415
35.012949	1257.911532	16.938432
35.252256	1259.389764	16.943450
35.505060	1256.340360	16.948467
35.157240	1270.584212	16.953485
35.532289	1259.883177	16.958503
35.718367	1255.065368	16.963520
35.526485	1258.367819	16.968538
35.367485	1260.834490	16.973555
35.388543	1264.798242	16.978573
35.720454	1252.104826	16.983591
35.511941	1263.460474	16.988608
35.521651	1261.351160	16.993626
35.441828	1257.741340	16.998643
35.132587	1260.066807	17.003661
35.316068	1254.285172	17.008679
34.963753	1248.400230	17.013696
35.375019	1278.342552	17.018714
35.518743	1291.163127	17.023731
35.752515	1297.356497	17.028749
35.972633	1292.397969	17.033767
35.580001	1292.487365	17.038784
35.720705	1296.413169	17.043802
36.009556	1293.855074	17.048819
35.672463	1293.068895	17.053837
36.128048	1298.726680	17.058855
35.842348	1282.528013	17.063872
35.843582	1287.138286	17.068890
35.898600	1291.080900	17.073907
35.809357	1299.293596	17.078925
36.311389	1308.056927	17.083943
36.215493	1316.552260	17.088960
36.691123	1313.885724	17.093978
37.017947	1285.636202	17.098995
36.539296	1287.468032	17.104013
36.499444	1285.750429	17.109031
36.499430	1280.005912	17.114048
36.398030	1278.471154	17.119066
36.501693	1269.941646	17.124083
36.562061	1289.047017	17.129101
36.803828	1281.904876	17.134119
36.713821	1286.375547	17.139136
36.749616	1264.338601	17.144154
36.800554	1270.789201	17.149171
36.644162	1276.649967	17.154189
36.984446	1274.542985	17.159207
36.667366	1274.044618	17.164224
36.536766	1272.667098	17.169242
36.820535	1275.362025	17.174259
36.751853	1273.240044	17.179277
36.863523	1278.296733	17.184295
36.609320	1274.378099	17.189312
36.656901	1273.670568	17.194330
36.846676	1279.174114	17.199347
36.606108	1275.415323	17.204365
36.439975	1283.788134	17.209383
36.723166	1278.788093	17.214400
36.821351	1294.478773	17.219418
37.130607	1303.869009	17.224435
37.143650	1305.282658	17.229453
37.156698	1299.339427	17.234471
37.083520	1306.478359	17.239488
36.943620	1306.944291	17.244506
36.942894	1301.053592	17.249523
36.777073	1301.605453	17.254541
37.035397	1298.767515	17.259559
37.158777	1299.553247	17.264576
37.487230	1320.272264	17.269594
37.485647	1325.476016	17.274611
37.566519	1329.436539	17.279629
37.649141	1324.621049	17.284647
37.426699	1320.338695	17.289664
37.633885	1327.631122	17.294682
37.918340	1328.065557	17.299699
37.799570	1324.682151	17.304717
38.005184	1301.292031	17.309735
37.625202	1296.901104	17.314752
37.555360	1303.883777	17.319770
37.756518	1299.489829	17.324787
37.759255	1303.047536	17.329805
37.706527	1307.367552	17.334823
37.738998	1312.408570	17.339840
37.790053	1321.133722	17.344858
38.121164	1317.008474	17.349875
38.038186	1341.445627	17.354893
38.456784	1310.084193	17.359911
38.227135	1325.292373	17.364928
38.116162	1279.477860	17.369946
38.002451	1308.840169	17.374963
37.805862	1296.001343	17.379981
37.887317	1321.121656	17.384999
38.417949	1312.280217	17.390016
38.360745	1311.136374	17.395034
38.300263	1322.304869	17.400051
38.284710	1330.306061	17.405069
38.302555	1326.893001	17.410087
38.324000	1322.924101	17.415104
38.430656	1322.108048	17.420122
38.371911	1315.949748	17.425139
38.453467	1321.324281	17.430157
38.332633	1323.515893	17.435175
38.159621	1323.938344	17.440192
38.096965	1320.033193	17.445210
38.454652	1309.932628	17.450227
38.489120	1316.846763	17.455245
38.461696	1314.667860	17.460263
38.441703	1330.621240	17.465280
38.744238	1344.078765	17.470298
39.062495	1341.062950	17.475315
39.253441	1343.574497	17.480333
39.102820	1332.112544	17.485351
38.919034	1318.242919	17.490368
38.677489	1313.509018	17.495386
39.063066	1335.856432	17.500403
39.271999	1341.731320	17.505421
38.891574	1331.882158	17.510439
39.299392	1326.656163	17.515456
38.894467	1334.335644	17.520474
39.586512	1339.335975	17.525491
39.149844	1332.652785	17.530509
39.428508	1343.090821	17.535527
39.276786	1317.377721	17.540544
39.170657	1308.309079	17.545562
39.510653	1321.343767	17.550579
39.444698	1322.436542	17.555597
39.259276	1301.246484	17.560615
39.563189	1334.661907	17.565632
39.340808	1329.058224	17.570650
39.548717	1348.730017	17.575667
39.424720	1341.016981	17.580685
39.317186	1352.446255	17.585703
39.836611	1344.673075	17.590720
39.181895	1340.157639	17.595738
39.572550	1356.039265	17.600755
39.660780	1325.584623	17.605773
39.359914	1353.171072	17.610791
39.564202	1328.118463	17.615808
39.518021	1329.865597	17.620826
39.560693	1347.619519	17.625843
39.862658	1337.450745	17.630861
40.183541	1351.281297	17.635879
40.123226	1362.196543	17.640896
39.997450	1337.583515	17.645914
39.929790	1358.401937	17.650931
40.104021	1333.580624	17.655949
39.910498	1366.301538	17.660967
40.129163	1363.554854	17.665984
39.734921	1366.065351	17.671002
40.233491	1367.849879	17.676019
40.518816	1364.526285	17.681037
40.098191	1348.226368	17.686055
40.553859	1373.376753	17.691072
40.689326	1350.954124	17.696090
40.380707	1373.138605	17.701107
40.483676	1355.868005	17.706125
40.354471	1347.471543	17.711143
40.403711	1372.419335	17.716160
40.762645	1355.540489	17.721178
40.659690	1358.806758	17.726195
40.660632	1363.859114	17.731213
40.468769	1360.998580	17.736231
40.956317	1358.668331	17.741248
40.674551	1364.657663	17.746266
40.746733	1368.317567	17.751283
40.825781	1368.920040	17.756301
40.716939	1365.185834	17.761319
40.738004	1365.467225	17.766336
40.766549	1367.885128	17.771354
40.960617	1360.771005	17.776371
40.977366	1372.490355	17.781389
40.893599	1350.357516	17.786407
40.764679	1366.021573	17.791424
40.977600	1380.552052	17.796442
41.237033	1393.192245	17.801459
41.097237	1393.494572	17.806477
41.439502	1394.525396	17.811495
41.276304	1384.971885	17.816512
41.128190	1399.100644	17.821530
41.479506	1399.890929	17.826547
41.476425	1393.893603	17.831565
41.474851	1385.612042	17.836583
41.857337	1393.062160	17.841600
41.552413	1391.273561	17.846618
41.533860	1394.023017	17.851635
41.932917	1388.611210	17.856653
41.796195	1390.377510	17.861671
41.702693	1354.826952	17.866688
41.510041	1375.202872	17.871706
41.753243	1369.573685	17.876723
41.739793	1360.916513	17.881741
41.684755	1382.206429	17.886759
42.062492	1402.975907	17.891776
41.720639	1370.187786	17.896794
41.880871	1394.746687	17.901811
42.033113	1377.526404	17.906829
41.959365	1395.322546	17.911847
41.905198	1385.899509	17.916864
41.650007	1379.789814	17.921882
41.815174	1402.995162	17.926899
41.861972	1376.533009	17.931917
41.503569	1395.765079	17.936935
42.232000	1378.723461	17.941952
41.886209	1393.541254	17.946970
41.985945	1388.518524	17.951987
42.233006	1412.558675	17.957005
42.223878	1426.745519	17.962023
42.415222	1391.920216	17.967040
42.083023	1421.658938	17.972058
42.353482	1407.798580	17.977075
42.365413	1409.673308	17.982093
42.402411	1437.250078	17.987111
42.500092	1401.050726	17.992128
42.392227	1411.753373	17.997146
42.339394	1428.476578	18.002163
42.699223	1417.598533	18.007181
42.573832	1453.630962	18.012199
43.181318	1430.020818	18.017216
42.873997	1440.432828	18.022234
42.807294	1436.533010	18.027251
42.953460	1419.947568	18.032269
42.876081	1448.141914	18.037287
43.655945	1419.316520	18.042304
42.995700	1431.721176	18.047322
42.937563	1400.146145	18.052339
43.106338	1401.965971	18.057357
42.999515	1438.033152	18.062375
43.151504	1422.422042	18.067392
42.949773	1440.631902	18.072410
42.852005	1433.586307	18.077427
42.777021	1431.210481	18.082445
42.462428	1431.822252	18.087463
43.236363	1430.346079	18.092480
43.136859	1454.098653	18.097498
43.237439	1458.820551	18.102515
43.658955	1459.804135	18.107533
43.749245	1456.848248	18.112551
44.015492	1429.779998	18.117568
44.000127	1448.518562	18.122586
44.071144	1450.270615	18.127603
44.131083	1430.842330	18.132621
43.449883	1422.332511	18.137639
43.585941	1407.592256	18.142656
43.560965	1448.241152	18.147674
44.096585	1429.427559	18.152691
44.110287	1446.988024	18.157709
44.067835	1445.531935	18.162727
44.236662	1422.782982	18.167744
43.722719	1436.406983	18.172762
43.904680	1434.171075	18.177779
44.357259	1440.754324	18.182797
44.340755	1452.644208	18.187815
44.324396	1438.596757	18.192832
44.294098	1427.299581	18.197850
44.061023	1434.210822	18.202867
44.414895	1439.713428	18.207885
44.016133	1441.703992	18.212903
44.452147	1430.521208	18.217920
44.319526	1451.788994	18.222938
44.491662	1452.192583	18.227955
44.613189	1438.651673	18.232973
44.400558	1434.180532	18.237991
44.658140	1452.085923	18.243008
44.930311	1440.539155	18.248026
44.328403	1436.803341	18.253043
44.666877	1452.164866	18.258061
44.808474	1442.504507	18.263079
45.319954	1439.454712	18.268096
44.949880	1434.716100	18.273114
44.821429	1443.540738	18.278131
45.070415	1446.302593	18.283149
45.028220	1435.885046	18.288167
44.744631	1444.624316	18.293184
44.833681	1447.222916	18.298202
45.250921	1447.343601	18.303219
45.317917	1430.695267	18.308237
45.048230	1437.966275	18.313255
45.093168	1433.918094	18.318272
44.837468	1446.940932	18.323290
44.783812	1453.886489	18.328307
44.854668	1441.187351	18.333325
44.911393	1462.146533	18.338343
45.234592	1465.137226	18.343360
45.177350	1472.618187	18.348378
45.405484	1477.584015	18.353395
45.403489	1469.939542	18.358413
45.348369	1469.306582	18.363431
45.402131	1471.486102	18.368448
45.366645	1474.170634	18.373466
45.382683	1482.069345	18.378483
45.740842	1495.779262	18.383501
45.690310	1491.867412	18.388519
45.970354	1495.338471	18.393536
46.086072	1493.050197	18.398554
46.065968	1493.248494	18.403571
45.991782	1487.210560	18.408589
46.066429	1499.386390	18.413607
46.237592	1500.044965	18.418624
46.402682	1485.410112	18.423642
46.178565	1486.090825	18.428659
46.488284	1489.915797	18.433677
46.231634	1479.878482	18.438695
46.269246	1471.011755	18.443712
46.366160	1461.696707	18.448730
46.492332	1463.163116	18.453747
46.447575	1463.974099	18.458765
46.110408	1466.933255	18.463783
46.086554	1466.690134	18.468800
46.337307	1483.924979	18.473818
46.340587	1486.659960	18.478835
46.564521	1484.519596	18.483853
46.327075	1491.925487	18.488871
46.659535	1487.013471	18.493888
46.577464	1483.123957	18.498906
46.189788	1492.803212	18.503923
46.531230	1488.978288	18.508941
46.441413	1512.748290	18.513959
47.073227	1512.315661	18.518976
47.299770	1513.572588	18.523994
47.101762	1524.906315	18.529011
47.081608	1515.383388	18.534029
46.918901	1513.647598	18.539047
46.877041	1514.966205	18.544064
47.097278	1519.653309	18.549082
46.885620	1522.276284	18.554099
47.117529	1509.279271	18.559117
47.010082	1520.568665	18.564135
47.311652	1518.371871	18.569152
47.280388	1517.109045	18.574170
47.006238	1522.562401	18.579187
47.471493	1514.854400	18.584205
47.172542	1519.918457	18.589223
47.379295	1530.339784	18.594240
47.857777	1530.762160	18.599258
47.809044	1538.820668	18.604275
48.121731	1535.705030	18.609293
47.743146	1521.804927	18.614311
47.787247	1509.229545	18.619328
48.356540	1510.456980	18.624346
47.738278	1525.351392	18.629363
47.676652	1506.404860	18.634381
47.685724	1504.039211	18.639399
48.094626	1521.706627	18.644416
48.045387	1532.980456	18.649434
48.287766	1543.314314	18.654451
48.441645	1530.973089	18.659469
47.985183	1534.638691	18.664487
48.187318	1532.462471	18.669504
48.451471	1529.401765	18.674522
48.195899	1532.421853	18.679539
48.397822	1540.366456	18.684557
48.498316	1540.325299	18.689575
48.485536	1529.427943	18.694592
48.845683	1525.439579	18.699610
48.614565	1524.476036	18.704627
48.696866	1529.955920	18.709645
48.752657	1537.635964	18.714663
48.524777	1526.865721	18.719680
48.838213	1531.191904	18.724698
48.408113	1525.531608	18.729715
48.591435	1545.737696	18.734733
48.784949	1530.906356	18.739751
48.646176	1529.644944	18.744768
48.770291	1553.829206	18.749786
48.818256	1531.725418	18.754803
48.940995	1524.924610	18.759821
49.138647	1536.892094	18.764839
48.744845	1537.470883	18.769856
48.870432	1525.131029	18.774874
48.551776	1530.651261	18.779891
48.913746	1566.768270	18.784909
49.054085	1560.246209	18.789927
48.914955	1568.098927	18.794944
49.305435	1564.695598	18.799962
48.992375	1571.533143	18.804979
49.251196	1564.304775	18.809997
49.048986	1566.079967	18.815015
49.380637	1582.001140	18.820032
49.733868	1578.698129	18.825050
49.497030	1580.274352	18.830067
49.955471	1580.454536	18.835085
50.111013	1575.394527	18.840103
50.109640	1576.606009	18.845120
50.168057	1575.409100	18.850138
50.061755	1577.612590	18.855155
49.964365	1571.210233	18.860173
50.123640	1575.191354	18.865191
49.789899	1576.619436	18.870208
50.214446	1568.142400	18.875226
49.949528	1581.643452	18.880243
50.217425	1575.365310	18.885261
50.443068	1579.217871	18.890279
50.311735	1575.254391	18.895296
50.376362	1576.895794	18.900314
50.496991	1578.194786	18.905331
50.650682	1578.388963	18.910349
50.462555	1582.093581	18.915367
50.351917	1576.168388	18.920384
50.570340	1572.589576	18.925402
50.460209	1567.120481	18.930419
50.226305	1570.373074	18.935437
50.433483	1577.708102	18.940455
50.086509	1575.915173	18.945472
50.370313	1578.602289	18.950490
49.994922	1597.820031	18.955507
50.528371	1595.806470	18.960525
50.705211	1605.018247	18.965543
50.430115	1615.568388	18.970560
50.811456	1602.748808	18.975578
51.035235	1616.775999	18.980595
51.206248	1621.345145	18.985613
51.388755	1620.746642	18.990631
51.179016	1605.754592	18.995648
51.454291	1588.300508	19.000666
51.161889	1590.775923	19.005683
51.470252	1591.774418	19.010701
51.646760	1596.592790	19.015719
51.506357	1585.549004	19.020736
51.742241	1576.337562	19.025754
51.594752	1590.727529	19.030771
51.532151	1591.627881	19.035789
51.621207	1594.223361	19.040807
51.569884	1592.732492	19.045824
51.580220	1601.923630	19.050842
51.529285	1603.518972	19.055859
51.849937	1605.495501	19.060877
51.984533	1612.579426	19.065895
51.529883	1635.526917	19.070912
52.156281	1620.068027	19.075930
52.263944	1623.867056	19.080947
52.486156	1624.350755	19.085965
52.295084	1611.691666	19.090983
52.174214	1601.670365	19.096000
52.107778	1592.458362	19.101018
52.007666	1614.674453	19.106035
52.117555	1615.100559	19.111053
52.284660	1617.019780	19.116071
52.181103	1616.284426	19.121088
52.576199	1605.902412	19.126106
52.400592	1615.126358	19.131123
52.356767	1614.523051	19.136141
52.562177	1617.192788	19.141159
52.507941	1618.890904	19.146176
52.543859	1621.164528	19.151194
52.589772	1621.769151	19.156211
52.646600	1614.407804	19.161229
52.778846	1615.253488	19.166247
52.932986	1642.942531	19.171264
53.328410	1632.066516	19.176282
52.732597	1632.507636	19.181299
52.820030	1627.766785	19.186317
53.107424	1638.496227	19.191335
53.166149	1644.182834	19.196352
53.561787	1642.781130	19.201370
53.539519	1643.808760	19.206387
53.643881	1637.913749	19.211405
53.407335	1621.889331	19.216423
53.075813	1619.942922	19.221440
53.526088	1622.716756	19.226458
53.924576	1634.145779	19.231475
53.667230	1614.116614	19.236493
53.751365	1602.126225	19.241511
53.487572	1609.012559	19.246528
53.504072	1611.314447	19.251546
53.699447	1632.866818	19.256563
53.848160	1635.710768	19.261581
54.097547	1619.520770	19.266599
53.681665	1636.382336	19.271616
53.920089	1625.779902	19.276634
53.558743	1632.274390	19.281651
53.779417	1631.418116	19.286669
54.105915	1634.343826	19.291687
53.682915	1642.394437	19.296704
53.914368	1631.330640	19.301722
53.766964	1635.790122	19.306739
53.924832	1638.234637	19.311757
54.374576	1643.042485	19.316775
54.227997	1652.375083	19.321792
54.595362	1658.297194	19.326810
54.263035	1660.014495	19.331827
54.564247	1660.836382	19.336845
54.964181	1666.404090	19.341863
54.712972	1660.345550	19.346880
54.705108	1646.895866	19.351898
54.569189	1657.224067	19.356915
54.614165	1655.573116	19.361933
54.867411	1647.010095	19.366951
54.611784	1659.893111	19.371968
54.776055	1657.537294	19.376986
54.802425	1652.233589	19.382003
54.564766	1655.040059	19.387021
54.530831	1666.394922	19.392039
54.813511	1680.598400	19.397056
55.146035	1682.972598	19.402074
55.140465	1684.419140	19.407091
55.400846	1691.992708	19.412109
55.603930	1687.172045	19.417127
55.107996	1689.366901	19.422144
55.457631	1690.311630	19.427162
55.248526	1686.594903	19.432179
55.259147	1681.882013	19.437197
55.525851	1682.325586	19.442215
55.441955	1695.890685	19.447232
55.592555	1706.901543	19.452250
55.754786	1710.089421	19.457267
55.978094	1708.921261	19.462285
56.031910	1711.025303	19.467303
55.788062	1715.855695	19.472320
56.136355	1705.364671	19.477338
56.579549	1701.735826	19.482355
56.365879	1708.607921	19.487373
56.716501	1695.815182	19.492391
56.177925	1668.300678	19.497408
56.217019	1682.912666	19.502426
56.603625	1657.240528	19.507443
56.257430	1686.086969	19.512461
56.674616	1660.623881	19.517479
56.098367	1663.245248	19.522496
56.263876	1689.636390	19.527514
56.418072	1667.030960	19.532531
56.642363	1696.220601	19.537549
56.809469	1693.247697	19.542567
56.622363	1710.088595	19.547584
56.432011	1693.878978	19.552602
56.688249	1697.935906	19.557619
56.643971	1701.689973	19.562637
57.025678	1698.140148	19.567655
56.761653	1686.996447	19.572672
56.870500	1708.605202	19.577690
56.840488	1701.767323	19.582707
56.630001	1689.119127	19.587725
57.017821	1722.849259	19.592743
57.164867	1728.224511	19.597760
57.349437	1719.614197	19.602778
57.295161	1733.618204	19.607795
57.424838	1734.689250	19.612813
57.698342	1719.937770	19.617831
57.335160	1724.299555	19.622848
56.910542	1737.236330	19.627866
57.272572	1735.330313	19.632883
57.378910	1733.795411	19.637901
57.401639	1727.885066	19.642919
57.470158	1745.680973	19.647936
57.877226	1756.377261	19.652954
58.049068	1753.579770	19.657971
58.021249	1748.317706	19.662989
57.955870	1747.297828	19.668007
57.979463	1747.427812	19.673024
58.285285	1759.650367	19.678042
58.369803	1737.284031	19.683059
58.405222	1736.642912	19.688077
58.388004	1752.063054	19.693095
58.140348	1738.160738	19.698112
58.253218	1750.001919	19.703130
58.537116	1742.775757	19.708147
58.292838	1737.227316	19.713165
58.366113	1739.244888	19.718183
58.560390	1752.674443	19.723200
58.635313	1727.699978	19.728218
58.455098	1736.545633	19.733235
58.649949	1746.655980	19.738253
58.798294	1740.267844	19.743271
58.959096	1755.423644	19.748288
58.973404	1770.846643	19.753306
59.307363	1752.689292	19.758323
58.888520	1764.215726	19.763341
59.330041	1770.484712	19.768359
59.201432	1768.504349	19.773376
59.270760	1769.154009	19.778394
59.375075	1767.012231	19.783411
59.374422	1779.381206	19.788429
59.607697	1761.897432	19.793447
59.175157	1767.228271	19.798464
59.230326	1767.284005	19.803482
59.610136	1770.294052	19.808499
59.444129	1773.534288	19.813517
59.707145	1777.129257	19.818535
59.731327	1744.521015	19.823552
59.467822	1755.852782	19.828570
59.802172	1756.702425	19.833587
59.263080	1759.346197	19.838605
59.670921	1766.429095	19.843623
59.639739	1773.611896	19.848640
59.838928	1785.725635	19.853658
60.545995	1774.260263	19.858675
60.278234	1785.913632	19.863693
60.358242	1789.981387	19.868711
60.357014	1788.523409	19.873728
60.156066	1790.809664	19.878746
60.272095	1784.392055	19.883763
60.107877	1782.470853	19.888781
60.814003	1785.907070	19.893799
60.473465	1787.792436	19.898816
60.496891	1789.401108	19.903834
60.810360	1781.471780	19.908851
60.903979	1773.489426	19.913869
60.751598	1789.152961	19.918887
60.592607	1771.961394	19.923904
60.400167	1790.752235	19.928922
60.908195	1793.024531	19.933939
60.816066	1781.088846	19.938957
60.926487	1774.596629	19.943975
60.954532	1810.850872	19.948992
60.987774	1817.183414	19.954010
61.496198	1809.060958	19.959027
61.185014	1816.687986	19.964045
61.308663	1818.324724	19.969063
61.359384	1800.624620	19.974080
61.527456	1815.795055	19.979098
61.683645	1807.326071	19.984115
61.337326	1800.818589	19.989133
61.663143	1807.255482	19.994151
61.562514	1795.948785	19.999168
61.127029	1816.755736	20.004186
61.628416	1798.474099	20.009203
61.345743	1806.996358	20.014221
61.625837	1830.040918	20.019239
61.918562	1833.948919	20.024256
62.084216	1825.837070	20.029274
62.116144	1814.564276	20.034291
61.921129	1844.601314	20.039309
62.438926	1828.407607	20.044327
62.298092	1817.997650	20.049344
62.029743	1840.336871	20.054362
62.437850	1801.710137	20.059379
62.262916	1820.919802	20.064397
62.567579	1852.061676	20.069415
62.693504	1850.253074	20.074432
62.783491	1866.150179	20.079450
62.963822	1846.824836	20.084467
62.849450	1858.790436	20.089485
62.993964	1826.365744	20.094503
62.567090	1846.367536	20.099520
62.535161	1830.182840	20.104538
62.783612	1860.754815	20.109555
62.970857	1859.128345	20.114573
63.115307	1847.623647	20.119591
63.090255	1838.167356	20.124608
63.175145	1866.687429	20.129626
63.474417	1841.082379	20.134643
63.554426	1840.251672	20.139661
63.397275	1837.413820	20.144679
63.837696	1833.124705	20.149696
63.571383	1841.350215	20.154714
63.887757	1836.380874	20.159731
63.832263	1839.976314	20.164749
63.687689	1842.580782	20.169767
64.074586	1836.097932	20.174784
63.613276	1829.877766	20.179802
63.786768	1834.391528	20.184819
63.618348	1838.829254	20.189837
64.060204	1838.491410	20.194855
63.752034	1839.092732	20.199872
63.508897	1829.350324	20.204890
63.585497	1848.383057	20.209907
63.787404	1863.738486	20.214925
64.075151	1872.745555	20.219943
64.540220	1861.737139	20.224960
63.857572	1855.258098	20.229978
63.936717	1875.333394	20.234995
64.262812	1876.459646	20.240013
64.583689	1885.492901	20.245031
64.951358	1892.223611	20.250048
65.005922	1898.099749	20.255066
65.174139	1886.109875	20.260083
64.955270	1886.140096	20.265101
65.110823	1892.114960	20.270119
65.132848	1888.496604	20.275136
65.065923	1886.139867	20.280154
65.349253	1882.245457	20.285171
65.152029	1889.901542	20.290189
65.219827	1884.300131	20.295207
65.538701	1885.347310	20.300224
65.271484	1887.587518	20.305242
65.644564	1879.999422	20.310259
65.604452	1883.560959	20.315277
65.398117	1890.321856	20.320295
65.801142	1890.032676	20.325312
65.715889	1877.472885	20.330330
65.699659	1873.022196	20.335347
65.757770	1901.697622	20.340365
65.721049	1882.973145	20.345383
65.714511	1868.736516	20.350400
65.340560	1904.081379	20.355418
65.784032	1873.131627	20.360435
65.491433	1895.454350	20.365453
65.645865	1898.228226	20.370471
66.323207	1880.401356	20.375488
66.064401	1896.843337	20.380506
66.180263	1905.387044	20.385523
66.055964	1902.990688	20.390541
66.021875	1896.202132	20.395559
66.478101	1897.376849	20.400576
66.520005	1923.660712	20.405594
66.513921	1908.736545	20.410611
66.413022	1943.153901	20.415629
66.538775	1923.237824	20.420647
67.142158	1919.484280	20.425664
66.774684	1915.611846	20.430682
67.105493	1932.878507	20.435699
66.740227	1935.458408	20.440717
67.058650	1904.122683	20.445735
67.093194	1930.533576	20.450752
66.670500	1904.985341	20.455770
66.911671	1940.476023	20.460787
67.335980	1938.569489	20.465805
67.453235	1938.879597	20.470823
67.702897	1941.908863	20.475840
67.746500	1957.044238	20.480858
67.991114	1932.199667	20.485875
67.488583	1952.891658	20.490893
67.727482	1928.132952	20.495911
67.679397	1959.697833	20.500928
67.758808	1943.852340	20.505946
67.565154	1938.744070	20.510963
67.947463	1950.254578	20.515981
67.955853	1947.698626	20.520999
68.010413	1945.007894	20.526016
67.887453	1944.255166	20.531034
68.017211	1948.895492	20.536051
68.084327	1963.928022	20.541069
68.302773	1967.709476	20.546087
68.636230	1958.921118	20.551104
68.601793	1979.607716	20.556122
68.739916	1972.799527	20.561139
68.740079	1964.334883	20.566157
68.653184	1988.556667	20.571175
68.756263	1967.473785	20.576192
68.754590	1970.365380	20.581210
68.732307	1970.186496	20.586227
68.614787	1964.864723	20.591245
68.607088	1979.335031	20.596263
68.962132	1969.690624	20.601280
68.945820	2003.336416	20.606298
69.373575	1987.642970	20.611315
69.630832	1988.970551	20.616333
69.488515	2001.618715	20.621351
69.825865	1999.188052	20.626368
69.380567	1984.599697	20.631386
69.740988	2001.108219	20.636403
69.574986	1978.597413	20.641421
69.517732	2003.229784	20.646439
69.835554	1965.464897	20.651456
69.633836	1989.719151	20.656474
69.890251	2000.897409	20.661491
69.818404	1985.168803	20.666509
70.014720	1983.287609	20.671527
70.335926	1990.618822	20.676544
69.973628	1988.688279	20.681562
70.182306	1979.101813	20.686579
70.265648	1984.249787	20.691597
69.772466	1996.889404	20.696615
70.453902	1977.792298	20.701632
70.011268	1979.988132	20.706650
70.044224	2011.257051	20.711667
70.478521	2016.281428	20.716685
70.732538	2007.820323	20.721703
70.768844	1996.041735	20.726720
70.604706	2029.501944	20.731738
70.702290	1998.372697	20.736755
70.730860	2026.488349	20.741773
70.914012	2022.504483	20.746791
70.790559	2000.444620	20.751808
70.586774	2022.929559	20.756826
70.951605	2040.112270	20.761843
71.325064	2035.648154	20.766861
71.127962	2029.631166	20.771879
71.425129	2032.965917	20.776896
71.373532	2042.901834	20.781914
71.509674	2037.874649	20.786931
71.535323	2022.643275	20.791949
71.491194	2039.639510	20.796967
72.011867	2039.968662	20.801984
71.818478	2035.673593	20.807002
71.922006	2046.987956	20.812019
71.960870	2038.683843	20.817037
72.082298	2063.301192	20.822055
72.184537	2063.094584	20.827072
72.378084	2055.612895	20.832090
72.243259	2058.132473	20.837107
72.349732	2055.184896	20.842125
72.446022	2052.968063	20.847143
72.593408	2056.631094	20.852160
72.544600	2053.765697	20.857178
72.522758	2038.217041	20.862195
72.936417	2057.374056	20.867213
72.645267	2024.806031	20.872231
72.864403	2056.952233	20.877248
72.939690	2025.309729	20.882266
72.720263	2067.814559	20.887283
72.949510	2041.768850	20.892301
73.055493	2037.114573	20.897319
73.033647	2063.222446	20.902336
73.010601	2037.247652	20.907354
73.103342	2046.533687	20.912371
73.397679	2038.238386	20.917389
73.291461	2086.834241	20.922407
73.414128	2070.377651	20.927424
73.896518	2036.850155	20.932442
73.872557	2080.859957	20.937459
73.835018	2059.696328	20.942477
73.915529	2039.738541	20.947495
74.066868	2079.064093	20.952512
73.903969	2044.492709	20.957530
73.901066	2011.273115	20.962547
74.262321	2031.437352	20.967565
74.018289	2056.094878	20.972583
74.116917	2073.611885	20.977600
73.827785	2061.256698	20.982618
73.854352	2053.208588	20.987635
74.251610	2058.022590	20.992653
74.058235	2069.627356	20.997671
74.095209	2047.036096	21.002688
74.045836	2091.576175	21.007706
74.223045	2073.329374	21.012723
74.111944	2102.372751	21.017741
74.785548	2068.226360	21.022759
74.769971	2089.734399	21.027776
74.591540	2115.444964	21.032794
74.975480	2093.891593	21.037811
75.324180	2125.733346	21.042829
75.194795	2116.329693	21.047847
75.513802	2104.963702	21.052864
75.333464	2131.110342	21.057882
75.415636	2092.713358	21.062899
75.438994	2123.829101	21.067917
75.498996	2107.996749	21.072935
75.281711	2116.625955	21.077952
75.526081	2112.996470	21.082970
75.353983	2114.409047	21.087987
76.037952	2097.642687	21.093005
75.719249	2133.760329	21.098023
76.040326	2116.808774	21.103040
76.021266	2152.169220	21.108058
76.190792	2124.741494	21.113075
76.083581	2139.315136	21.118093
76.264902	2156.491856	21.123111
76.592053	2131.564568	21.128128
76.304581	2143.634299	21.133146
76.400163	2137.594189	21.138163
76.642598	2124.650795	21.143181
76.401193	2150.221235	21.148199
76.521751	2136.964557	21.153216
76.492832	2114.987763	21.158234
76.113570	2152.209971	21.163251
76.715531	2149.452360	21.168269
76.678248	2158.523237	21.173287
76.973469	2164.826740	21.178304
76.750378	2156.523432	21.183322
76.879289	2173.486724	21.188339
77.469146	2169.474930	21.193357
77.124524	2166.457688	21.198375
77.532737	2200.012642	21.203392
78.165843	2167.227695	21.208410
77.961039	2174.089942	21.213427
78.454275	2141.302974	21.218445
77.907464	2139.600040	21.223463
77.511372	2153.316027	21.228480
78.025306	2141.842630	21.233498
77.847178	2153.611778	21.238515
78.122254	2147.565064	21.243533
77.978120	2139.679413	21.248551
78.064326	2147.847307	21.253568
77.696785	2159.952629	21.258586
78.002866	2162.055051	21.263603
78.046546	2172.181151	21.268621
78.146931	2184.590203	21.273639
78.572082	2182.687438	21.278656
78.390974	2172.021729	21.283674
78.317752	2173.067747	21.288691
78.518707	2186.227643	21.293709
78.663362	2167.086896	21.298727
78.677411	2219.658868	21.303744
78.937456	2193.514378	21.308762
79.042068	2219.121787	21.313779
79.213672	2186.101278	21.318797
78.631213	2215.129591	21.323815
79.092394	2192.939240	21.328832
78.963504	2210.955182	21.333850
79.526852	2216.497049	21.338867
79.895418	2230.510401	21.343885
80.081123	2201.852152	21.348903
79.922729	2220.469011	21.353920
80.100083	2179.962833	21.358938
80.079864	2197.479279	21.363955
80.119677	2175.489073	21.368973
79.807713	2191.580411	21.373991
79.892986	2177.888072	21.379008
80.122534	2190.604522	21.384026
80.025990	2239.236311	21.389043
80.477190	2196.650051	21.394061
80.347810	2232.556842	21.399079
80.325121	2214.614672	21.404096
80.768717	2228.877192	21.409114
80.264412	2215.432997	21.414131
80.431501	2210.081480	21.419149
80.234768	2205.933976	21.424167
80.672903	2235.821306	21.429184
80.998746	2219.016743	21.434202
80.790382	2241.065429	21.439219
80.816285	2229.126283	21.444237
80.854358	2255.099885	21.449255
81.025897	2230.755691	21.454272
81.337016	2233.812187	21.459290
81.233442	2248.994146	21.464307
81.317364	2237.349348	21.469325
81.343398	2231.336808	21.474343
81.409813	2256.019103	21.479360
81.821368	2242.881887	21.484378
81.260981	2271.527677	21.489395
81.849977	2265.175229	21.494413
81.682148	2246.631645	21.499431
81.687340	2262.397196	21.504448
81.902008	2259.687166	21.509466
81.742114	2245.047529	21.514483
82.228507	2258.176131	21.519501
82.333766	2246.055996	21.524519
82.179687	2276.505841	21.529536
82.541196	2275.495721	21.534554
82.567876	2279.529644	21.539571
82.699780	2280.942526	21.544589
82.748867	2282.877512	21.549607
82.744421	2277.719285	21.554624
82.655448	2265.877082	21.559642
83.091034	2286.163535	21.564659
82.623720	2282.811098	21.569677
83.022317	2255.010742	21.574695
82.800060	2303.006024	21.579712
83.323677	2258.515596	21.584730
83.361405	2283.787704	21.589747
82.769951	2283.541481	21.594765
83.449828	2291.408711	21.599783
83.322266	2308.631720	21.604800
83.959348	2299.264608	21.609818
84.165857	2296.672283	21.614835
84.184300	2285.011146	21.619853
84.386954	2295.609868	21.624871
83.959461	2302.969390	21.629888
84.645958	2284.890449	21.634906
84.277356	2294.900685	21.639923
84.262265	2294.845711	21.644941
84.305632	2285.848575	21.649959
84.162734	2290.778679	21.654976
84.651653	2293.970439	21.659994
84.768767	2270.014761	21.665011
84.623440	2304.352750	21.670029
84.779497	2275.296370	21.675047
84.557803	2302.834238	21.680064
84.771184	2270.228467	21.685082
84.474440	2290.195956	21.690099
84.830599	2285.050227	21.695117
84.765285	2282.686089	21.700135
85.118183	2295.958716	21.705152
85.395972	2305.427777	21.710170
85.227446	2325.909723	21.715187
85.409129	2310.706652	21.720205
85.343814	2308.343296	21.725223
85.046728	2311.675341	21.730240
85.415226	2307.438462	21.735258
85.482781	2321.822389	21.740275
85.610960	2325.206967	21.745293
85.615152	2348.613330	21.750311
85.701868	2343.766176	21.755328
86.123430	2325.286603	21.760346
86.034824	2352.087581	21.765363
86.402294	2331.035161	21.770381
86.518320	2330.783877	21.775399
86.055405	2331.774064	21.780416
86.171200	2328.195705	21.785434
86.226195	2353.034937	21.790451
86.276858	2361.160639	21.795469
86.883681	2363.359860	21.800487
86.670648	2360.617336	21.805504
86.800142	2353.435947	21.810522
86.828102	2362.881959	21.815539
86.627518	2364.555518	21.820557
87.183044	2375.873571	21.825575
87.084042	2387.797040	21.830592
87.218058	2384.790733	21.835610
87.495920	2392.928990	21.840627
87.845696	2379.091245	21.845645
88.089468	2393.555688	21.850663
87.933411	2379.214193	21.855680
88.047184	2379.928371	21.860698
87.745840	2390.926871	21.865715
88.041941	2381.234175	21.870733
88.426693	2376.885354	21.875751
88.229946	2378.865845	21.880768
88.117335	2369.754310	21.885786
88.350196	2394.625028	21.890803
88.304724	2360.968592	21.895821
88.601910	2386.386705	21.900839
88.730680	2369.279110	21.905856
88.760216	2391.040750	21.910874
88.607874	2373.520201	21.915891
88.152766	2378.595293	21.920909
88.329684	2376.743887	21.925927
88.317016	2379.141788	21.930944
88.672221	2407.311491	21.935962
88.940786	2386.664108	21.940979
88.501998	2407.439389	21.945997
89.333242	2382.027788	21.951015
88.993882	2411.419655	21.956032
89.166201	2418.987200	21.961050
89.012632	2419.250838	21.966067
89.173241	2448.236634	21.971085
89.301733	2408.273259	21.976103
89.365537	2465.097383	21.981120
89.753913	2435.661486	21.986138
89.968420	2454.042991	21.991155
89.894816	2449.534417	21.996173
89.768444	2440.442336	22.001191
90.216452	2449.295217	22.006208
90.553961	2425.876753	22.011226
90.335482	2457.104924	22.016243
90.344692	2459.432492	22.021261
90.946019	2433.233939	22.026279
90.802761	2477.905009	22.031296
90.324590	2450.531185	22.036314
90.934798	2437.829334	22.041331
91.282795	2425.474490	22.046349
91.370669	2460.533902	22.051367
91.100149	2475.048186	22.056384
91.484179	2439.952893	22.061402
91.154797	2468.920117	22.066419
91.278638	2432.330183	22.071437
91.761858	2447.871836	22.076455
91.209812	2478.517704	22.081472
90.969536	2454.560507	22.086490
91.830675	2445.134766	22.091507
91.733618	2481.059040	22.096525
91.361434	2465.838728	22.101543
91.405007	2458.981678	22.106560
91.920999	2471.425384	22.111578
92.043553	2500.494435	22.116595
92.288018	2473.489858	22.121613
92.754775	2477.227920	22.126631
92.280438	2510.190465	22.131648
92.404102	2476.321950	22.136666
92.297418	2498.652918	22.141683
92.512155	2466.461795	22.146701
92.516039	2496.462956	22.151719
92.304950	2485.860001	22.156736
93.272455	2481.909038	22.161754
93.081469	2529.056101	22.166771
93.074704	2505.358905	22.171789
93.379513	2527.820941	22.176807
93.436301	2500.942200	22.181824
93.354172	2519.147707	22.186842
93.152930	2504.649688	22.191859
93.323106	2528.949364	22.196877
93.149214	2513.443322	22.201895
93.420511	2503.370659	22.206912
93.810257	2541.710856	22.211930
94.051065	2563.133091	22.216947
93.822616	2550.651396	22.221965
93.956355	2518.670501	22.226983
93.867604	2557.934954	22.232000
94.094095	2529.991622	22.237018
94.492322	2570.186042	22.242035
94.431851	2577.629544	22.247053
94.629177	2565.696609	22.252071
94.692403	2551.117831	22.257088
94.917253	2530.562951	22.262106
95.170289	2577.567791	22.267123
94.644037	2567.885758	22.272141
95.227762	2543.881969	22.277159
95.147377	2555.767997	22.282176
95.290720	2585.199655	22.287194
95.108715	2558.701827	22.292211
95.269414	2543.458599	22.297229
95.281366	2575.937097	22.302247
95.560394	2554.158302	22.307264
95.504758	2577.552550	22.312282
95.753986	2564.168781	22.317299
95.638434	2590.132082	22.322317
96.297674	2559.535035	22.327335
95.968291	2586.035040	22.332352
95.957916	2555.555001	22.337370
96.199886	2577.673182	22.342387
96.274093	2556.258974	22.347405
96.213720	2584.379664	22.352423
96.318952	2545.361926	22.357440
96.176821	2583.415788	22.362458
96.330566	2599.538713	22.367475
96.465747	2570.277421	22.372493
96.811467	2614.078868	22.377511
96.453499	2595.673703	22.382528
96.583506	2609.782097	22.387546
96.838153	2595.543224	22.392563
96.957699	2642.654509	22.397581
97.049025	2612.455457	22.402599
96.956621	2624.171986	22.407616
97.172822	2602.024799	22.412634
97.246811	2663.030245	22.417651
97.433247	2636.973783	22.422669
97.671671	2668.145280	22.427687
97.974049	2656.326878	22.432704
98.133865	2620.372575	22.437722
98.316707	2610.790603	22.442739
98.134277	2658.442482	22.447757
98.513285	2656.716131	22.452775
98.352235	2643.793355	22.457792
98.663740	2619.374280	22.462810
99.063505	2646.234001	22.467827
98.533716	2650.463733	22.472845
98.907603	2628.318893	22.477863
98.842714	2642.452104	22.482880
98.452922	2639.176101	22.487898
99.200671	2654.601072	22.492915
99.082173	2666.646649	22.497933
99.194833	2648.232444	22.502951
99.420217	2685.689957	22.507968
98.909137	2660.344043	22.512986
99.523958	2635.812076	22.518003
99.173684	2682.926830	22.523021
99.557127	2658.557571	22.528039
99.523357	2702.728919	22.533056
99.848192	2686.296030	22.538074
100.240485	2684.051567	22.543091
100.073837	2704.112930	22.548109
100.189204	2676.697521	22.553127
100.070178	2699.342246	22.558144
100.288938	2673.326185	22.563162
100.405635	2725.985873	22.568179
100.030661	2733.330941	22.573197
100.055363	2717.089819	22.578215
100.883342	2688.159087	22.583232
100.801784	2731.222784	22.588250
101.038793	2692.259939	22.593267
100.949124	2690.027041	22.598285
101.130193	2723.570663	22.603303
101.043064	2755.471497	22.608320
101.060203	2761.714990	22.613338
101.814625	2722.946434	22.618355
101.719935	2749.148957	22.623373
101.648203	2761.397170	22.628391
101.596180	2738.880380	22.633408
101.359112	2750.463549	22.638426
101.038955	2747.037980	22.643443
101.340525	2749.932504	22.648461
102.393274	2727.197883	22.653479
102.301255	2784.886590	22.658496
102.004501	2786.430800	22.663514
102.520574	2742.455310	22.668531
102.369782	2785.047249	22.673549
102.209252	2766.428685	22.678567
102.907761	2775.628820	22.683584
102.689029	2798.633330	22.688602
102.934520	2775.005593	22.693619
103.012645	2779.515196	22.698637
102.861552	2817.660766	22.703655
103.139516	2777.913238	22.708672
103.087472	2794.636315	22.713690
103.376284	2773.985157	22.718707
103.355705	2795.719210	22.723725
103.090448	2803.448759	22.728743
103.837070	2798.569381	22.733760
103.712855	2833.972635	22.738778
103.946477	2787.897047	22.743795
104.330854	2822.170669	22.748813
104.687318	2789.689585	22.753831
104.244024	2815.988716	22.758848
104.365217	2794.454973	22.763866
104.798391	2819.734962	22.768883
104.544038	2795.010174	22.773901
104.564782	2806.821288	22.778919
104.070626	2818.289762	22.783936
104.629274	2795.587414	22.788954
104.725586	2850.958988	22.793971
104.706482	2823.899041	22.798989
105.067141	2843.877301	22.804007
105.527278	2833.208751	22.809024
105.046889	2831.164772	22.814042
105.642745	2846.438763	22.819059
105.479187	2823.823999	22.824077
105.756815	2864.235895	22.829095
105.843790	2847.988630	22.834112
105.863082	2854.647133	22.839130
106.235933	2846.355377	22.844147
105.837746	2837.385833	22.849165
106.074005	2852.258594	22.854183
106.715929	2851.652077	22.859200
106.128623	2843.732878	22.864218
106.258690	2854.091092	22.869235
106.153186	2857.465861	22.874253
106.183212	2841.735028	22.879271
106.179830	2864.369434	22.884288
106.241813	2894.566661	22.889306
106.359204	2872.668435	22.894323
106.460712	2889.538611	22.899341
107.011009	2912.586646	22.904359
107.192187	2899.418720	22.909376
107.095859	2925.648564	22.914394
107.522784	2881.992064	22.919411
107.673926	2915.558205	22.924429
107.385668	2895.635236	22.929447
107.804197	2935.767651	22.934464
107.798007	2919.772709	22.939482
108.153316	2922.138769	22.944499
108.361455	2933.062729	22.949517
108.523730	2915.453604	22.954535
108.769709	2930.310736	22.959552
108.696022	2914.882678	22.964570
108.587442	2947.422125	22.969587
108.635145	2918.386462	22.974605
108.761197	2888.270185	22.979623
109.055571	2893.517766	22.984640
108.852987	2945.956215	22.989658
109.148169	2927.924725	22.994675
108.925341	2933.840793	22.999693
109.137023	2908.766197	23.004711
109.813334	2886.713542	23.009728
109.243807	2921.679097	23.014746
109.073173	2958.790648	23.019763
109.496641	2936.310217	23.024781
109.372690	2940.674324	23.029799
109.476828	2965.817466	23.034816
109.690017	2947.038398	23.039834
110.118243	2970.039916	23.044851
110.172003	2952.658854	23.049869
110.265561	2988.931545	23.054887
110.304440	2958.563158	23.059904
110.356741	2962.997491	23.064922
110.740239	2944.719068	23.069939
110.783614	2995.762406	23.074957
110.648847	2978.527789	23.079975
111.112380	2972.546653	23.084992
111.226163	2984.302960	23.090010
111.229474	2967.389291	23.095027
111.116940	2978.959863	23.100045
111.240036	2980.282189	23.105063
111.106556	2985.602745	23.110080
111.349384	2992.988658	23.115098
111.493591	3010.112526	23.120115
112.094138	3007.297571	23.125133
111.901246	2999.707116	23.130151
112.067942	3023.194055	23.135168
112.000998	3003.672993	23.140186
112.303192	2995.858080	23.145203
112.583506	2994.238673	23.150221
112.091123	3004.200694	23.155239
112.788668	2996.562651	23.160256
112.674721	3039.679618	23.165274
112.771263	3011.393468	23.170291
113.170246	3018.676623	23.175309
112.913182	3017.639236	23.180327
112.792858	3023.855205	23.185344
112.984109	3013.815408	23.190362
112.853082	3031.346591	23.195379
113.480422	3010.001625	23.200397
113.613086	3069.126550	23.205415
113.905909	3058.361021	23.210432
113.986831	3041.488380	23.215450
113.523382	3062.743620	23.220467
114.037402	3026.846681	23.225485
114.092386	3024.766863	23.230503
114.404015	3056.581177	23.235520
113.998229	3068.888419	23.240538
114.357952	3033.959188	23.245555
114.659357	3073.910867	23.250573
114.519509	3088.876091	23.255591
115.288955	3056.865807	23.260608
115.030063	3095.351794	23.265626
114.784312	3066.139235	23.270643
115.091476	3094.918103	23.275661
114.921261	3065.215254	23.280679
115.130723	3085.179412	23.285696
115.299315	3071.491828	23.290714
115.430660	3111.786149	23.295731
115.569059	3087.478848	23.300749
115.381096	3116.525488	23.305767
115.660180	3073.891750	23.310784
115.614210	3115.715958	23.315802
115.893593	3113.067823	23.320819
115.941430	3114.465876	23.325837
115.921515	3133.968761	23.330855
116.443036	3101.423698	23.335872
116.350929	3149.432476	23.340890
116.447771	3139.075703	23.345907
117.214353	3122.451541	23.350925
117.499543	3109.783634	23.355943
117.480599	3127.814640	23.360960
117.331573	3155.455798	23.365978
117.481720	3126.828933	23.370995
117.542778	3148.634661	23.376013
117.536522	3148.666374	23.381031
117.493236	3128.829879	23.386048
117.580929	3143.365581	23.391066
117.583536	3116.489625	23.396083
118.066615	3161.805466	23.401101
117.974200	3142.883732	23.406119
118.404357	3172.807304	23.411136
118.104887	3153.903625	23.416154
118.612719	3153.141497	23.421171
118.240402	3152.706131	23.426189
118.538433	3183.081060	23.431207
118.165893	3151.124444	23.436224
118.592253	3136.558760	23.441242
118.521638	3202.245377	23.446259
118.574227	3201.346600	23.451277
118.646002	3173.829445	23.456295
119.045329	3213.705325	23.461312
119.378060	3214.791305	23.466330
119.420583	3192.383022	23.471347
119.618004	3234.279672	23.476365
119.521380	3207.027645	23.481383
119.849872	3225.565792	23.486400
119.536540	3219.082294	23.491418
119.684692	3217.989720	23.496435
119.873319	3241.351591	23.501453
120.162832	3216.015493	23.506471
120.560683	3217.697558	23.511488
120.650478	3273.166953	23.516506
120.528488	3269.641225	23.521523
121.189183	3234.576215	23.526541
121.311356	3245.889326	23.531559
121.217592	3278.024408	23.536576
120.861383	3281.356655	23.541594
121.225521	3248.343161	23.546611
121.658402	3275.381258	23.551629
121.313040	3262.275723	23.556647
121.754821	3237.842712	23.561664
121.703309	3275.807628	23.566682
122.176372	3261.574187	23.571699
122.109647	3298.080867	23.576717
122.471210	3260.395331	23.581735
122.581075	3302.613700	23.586752
122.244062	3278.079829	23.591770
122.396966	3289.399873	23.596787
122.851287	3285.184432	23.601805
122.484339	3272.920848	23.606823
122.758125	3277.548863	23.611840
122.998207	3291.580587	23.616858
122.673042	3288.308286	23.621875
123.082443	3289.658145	23.626893
122.916693	3296.061604	23.631911
123.188170	3300.513796	23.636928
123.203022	3317.581564	23.641946
123.256900	3304.929919	23.646963
123.993307	3307.125156	23.651981
123.946513	3324.462340	23.656999
124.073621	3330.753831	23.662016
123.887783	3307.544835	23.667034
123.843659	3344.120394	23.672051
124.644407	3313.783966	23.677069
124.312820	3376.605687	23.682087
124.242946	3344.356539	23.687104
124.668070	3340.272382	23.692122
124.484382	3368.950710	23.697139
124.953551	3349.602498	23.702157
124.799046	3386.758973	23.707175
125.040634	3366.651764	23.712192
125.078686	3393.911143	23.717210
125.148831	3359.063494	23.722227
125.502977	3387.773308	23.727245
125.869386	3396.679903	23.732263
125.827697	3392.800740	23.737280
126.093584	3397.153954	23.742298
125.711948	3396.099429	23.747315
126.185194	3404.893815	23.752333
126.252572	3402.426529	23.757351
126.041779	3387.611361	23.762368
126.656815	3416.866445	23.767386
126.395183	3432.512190	23.772403
127.124169	3420.243648	23.777421
127.118610	3424.121774	23.782439
127.159748	3412.392402	23.787456
127.034241	3435.019634	23.792474
127.085317	3410.683243	23.797491
127.680891	3419.189113	23.802509
127.745779	3451.131730	23.807527
128.119447	3449.049023	23.812544
128.028571	3431.458403	23.817562
128.188387	3449.473103	23.822579
128.338899	3427.663944	23.827597
128.237572	3444.290217	23.832615
128.110695	3446.933834	23.837632
128.656017	3429.869494	23.842650
128.049742	3444.411525	23.847667
128.380430	3452.304402	23.852685
128.635811	3454.200359	23.857703
128.603772	3462.660014	23.862720
128.869286	3481.066938	23.867738
129.017382	3461.693470	23.872755
129.433372	3480.052016	23.877773
129.345000	3507.685741	23.882791
129.485362	3477.972648	23.887808
129.778833	3504.269598	23.892826
129.549679	3497.657706	23.897843
130.093989	3485.812650	23.902861
130.293366	3494.137099	23.907879
129.966127	3518.488631	23.912896
130.262501	3523.231903	23.917914
130.347494	3514.910943	23.922931
130.502110	3515.073542	23.927949
130.329945	3523.830890	23.932967
130.648980	3521.201533	23.937984
130.787497	3533.501038	23.943002
130.816063	3544.498141	23.948019
130.853320	3548.454427	23.953037
131.576167	3554.104331	23.958055
131.223291	3560.921610	23.963072
131.594927	3571.737388	23.968090
131.838834	3555.487914	23.973107
131.998596	3583.396865	23.978125
131.970055	3551.014026	23.983143
132.250907	3570.703950	23.988160
132.180534	3561.260846	23.993178
132.415319	3579.668861	23.998195
132.416957	3538.327159	24.003213
132.518211	3576.450206	24.008231
131.972800	3589.436970	24.013248
132.366786	3599.479891	24.018266
132.562051	3582.176207	24.023283
132.874779	3614.848193	24.028301
133.080691	3614.501538	24.033319
132.905742	3602.961430	24.038336
133.523034	3627.623506	24.043354
133.573919	3621.961984	24.048371
133.849323	3654.814640	24.053389
134.292042	3626.570434	24.058407
134.163562	3635.310656	24.063424
134.442771	3634.211317	24.068442
134.598726	3660.539126	24.073459
134.795607	3626.085972	24.078477
134.742110	3662.152516	24.083495
134.636632	3638.490458	24.088512
134.901776	3647.674513	24.093530
134.547234	3636.168520	24.098547
135.089919	3663.583143	24.103565
135.311678	3667.420370	24.108583
135.474328	3670.125632	24.113600
135.509064	3654.617360	24.118618
135.469924	3660.353400	24.123635
135.481382	3661.731347	24.128653
135.852399	3669.827941	24.133671
136.093748	3679.525542	24.138688
136.278918	3676.299216	24.143706
135.989402	3687.594141	24.148723
136.076097	3664.444958	24.153741
136.249417	3702.457730	24.158759
136.442778	3694.175240	24.163776
136.753206	3722.993373	24.168794
136.846899	3700.270943	24.173811
137.033646	3727.746371	24.178829
137.168212	3732.563495	24.183847
137.243699	3747.230751	24.188864
137.724629	3735.869151	24.193882
137.787855	3738.474643	24.198899
137.373989	3729.824839	24.203917
137.675541	3739.004720	24.208935
137.923743	3759.159496	24.213952
138.195081	3772.449629	24.218970
138.216672	3746.220818	24.223987
138.614520	3790.887505	24.229005
138.420528	3759.163821	24.234023
138.574544	3771.280917	24.239040
139.021176	3764.094686	24.244058
138.576541	3793.479364	24.249075
138.819832	3791.665187	24.254093
139.192275	3778.004226	24.259111
138.870088	3803.249823	24.264128
139.500742	3788.100283	24.269146
139.443786	3813.473521	24.274163
139.688955	3833.328389	24.279181
139.880970	3806.255774	24.284199
139.696810	3816.010296	24.289216
140.043106	3807.653801	24.294234
140.049349	3851.251933	24.299251
140.475449	3823.708529	24.304269
140.702464	3850.236169	24.309287
140.966032	3836.087494	24.314304
140.980214	3839.469365	24.319322
141.001340	3817.620472	24.324339
141.125192	3847.256016	24.329357
141.576672	3854.798682	24.334375
141.307953	3851.723348	24.339392
141.562459	3859.888183	24.344410
141.559567	3874.431189	24.349427
141.551449	3866.251523	24.354445
141.629640	3848.638164	24.359463
141.369754	3893.459590	24.364480
141.998782	3877.116893	24.369498
142.138855	3883.401836	24.374515
142.456016	3916.747151	24.379533
142.815154	3901.200270	24.384551
142.507511	3915.426119	24.389568
142.763303	3911.840002	24.394586
142.764311	3911.894943	24.399603
143.314377	3931.857875	24.404621
143.436663	3932.003609	24.409639
143.480015	3945.115498	24.414656
143.682601	3940.029085	24.419674
143.785628	3932.586834	24.424691
143.484559	3938.074474	24.429709
143.994218	3961.659277	24.434727
144.205608	3973.875950	24.439744
144.414999	3956.030725	24.444762
144.350583	3979.222516	24.449779
144.574275	3958.093146	24.454797
145.043626	4004.762882	24.459815
145.056017	3974.088246	24.464832
145.096346	4001.586746	24.469850
145.263178	3996.748300	24.474867
145.399245	3977.243127	24.479885
145.231375	3997.847663	24.484903
145.545924	4005.747349	24.489920
145.605349	4005.539678	24.494938
145.911973	4014.417641	24.499955
145.632916	4034.346137	24.504973
145.865279	4008.662221	24.509991
146.065890	4048.247184	24.515008
146.416440	4050.629927	24.520026
146.538088	4021.105153	24.525043
147.106191	4051.759782	24.530061
146.934781	4027.471998	24.535079
146.685151	4046.935634	24.540096
147.244150	4046.035517	24.545114
147.255511	4073.301990	24.550131
147.725407	4056.652503	24.555149
148.157579	4083.679628	24.560167
148.083823	4052.382953	24.565184
148.095213	4077.154194	24.570202
148.552129	4039.727569	24.575219
148.562248	4060.297522	24.580237
148.739461	4039.736322	24.585255
148.235207	4058.899166	24.590272
148.846130	4035.718522	24.595290
148.523695	4061.302857	24.600307
148.790952	4046.492611	24.605325
149.017903	4074.366616	24.610343
149.050695	4047.100255	24.615360
149.657136	4056.454348	24.620378
149.586668	4082.685289	24.625395
149.834149	4042.685103	24.630413
149.893458	4072.071015	24.635431
149.828084	4072.197899	24.640448
149.952253	4096.465832	24.645466
150.106398	4080.216717	24.650483
149.594680	4095.972264	24.655501
150.577563	4101.237951	24.660519
150.298961	4106.980092	24.665536
150.486492	4125.946984	24.670554
150.341540	4114.269532	24.675571
150.645060	4158.511072	24.680589
151.141182	4130.334478	24.685607
150.948244	4170.525304	24.690624
151.231032	4173.862853	24.695642
151.879775	4151.007965	24.700659
151.412934	4182.106347	24.705677
151.760932	4172.444322	24.710695
151.937971	4207.310423	24.715712
152.285967	4182.945076	24.720730
152.514345	4208.666045	24.725747
152.628507	4199.071176	24.730765
153.098668	4226.174321	24.735783
153.022835	4204.148367	24.740800
153.023804	4233.679995	24.745818
153.195257	4209.597627	24.750835
152.823974	4239.313693	24.755853
153.570896	4238.090971	24.760871
153.312275	4247.869449	24.765888
153.801527	4264.437106	24.770906
153.924341	4242.959975	24.775923
153.833561	4277.900409	24.780941
154.497052	4254.781840	24.785959
154.438022	4309.031254	24.790976
154.522168	4273.824415	24.795994
154.039122	4296.366020	24.801011
154.289342	4264.484673	24.806029
154.703896	4319.467302	24.811047
154.786962	4294.476137	24.816064
154.927042	4314.255588	24.821082
155.474105	4303.302300	24.826099
155.374554	4349.079729	24.831117
155.962057	4323.433829	24.836135
156.023788	4345.480378	24.841152
156.074060	4337.082675	24.846170
156.571137	4322.198539	24.851187
156.123087	4333.380781	24.856205
156.818310	4336.971997	24.861223
156.612762	4337.421735	24.866240
157.041226	4370.114718	24.871258
157.440367	4333.241714	24.876275
157.136952	4360.622627	24.881293
158.079188	4324.596037	24.886311
157.652915	4365.289512	24.891328
157.368877	4331.440013	24.896346
157.844608	4351.356373	24.901363
157.970496	4337.485620	24.906381
158.225767	4369.056904	24.911399
157.986696	4372.489501	24.916416
158.352841	4373.357064	24.921434
158.429603	4383.661931	24.926451
158.321451	4365.243800	24.931469
158.879019	4397.233439	24.936487
158.707224	4390.664701	24.941504
158.816094	4400.127452	24.946522
159.169321	4411.989908	24.951539
159.547876	4419.800949	24.956557
159.420134	4411.451251	24.961575
159.721095	4437.541009	24.966592
159.913750	4424.249528	24.971610
160.301247	4441.805140	24.976627
160.247788	4445.935826	24.981645
160.623627	4445.609264	24.986663
160.643194	4446.963180	24.991680
160.694402	4451.859912	24.996698
160.920618	4444.108270	25.001715
160.965359	4463.707244	25.006733
161.274690	4462.410312	25.011751
161.453177	4473.041224	25.016768
161.488229	4474.225113	25.021786
161.688198	4454.759466	25.026803
161.901329	4481.546131	25.031821
162.217536	4499.254778	25.036839
162.396311	4502.095293	25.041856
162.130468	4489.694200	25.046874
162.622851	4495.439438	25.051891
162.656252	4496.673153	25.056909
162.969524	4493.089533	25.061927
162.839363	4510.464225	25.066944
162.971097	4515.934996	25.071962
163.175538	4528.924178	25.076979
163.112644	4536.313993	25.081997
163.322178	4517.070152	25.087015
163.399116	4536.920545	25.092032
163.426215	4544.024616	25.097050
163.609029	4559.136563	25.102067
164.079343	4557.877679	25.107085
164.615085	4561.681607	25.112103
164.607587	4577.077222	25.117120
164.597220	4588.237863	25.122138
164.965129	4577.880128	25.127155
164.695141	4570.522984	25.132173
164.721224	4601.233715	25.137191
164.925377	4608.533791	25.142208
165.131569	4595.582201	25.147226
165.231208	4638.654086	25.152243
165.410762	4619.482546	25.157261
165.663858	4648.243204	25.162279
166.054880	4642.097537	25.167296
166.058824	4658.543985	25.172314
166.512971	4642.565025	25.177331
166.397045	4665.335800	25.182349
166.756192	4667.035230	25.187367
167.352764	4676.760251	25.192384
167.356913	4680.637162	25.197402
167.624198	4690.358049	25.202419
167.796656	4694.201836	25.207437
167.798887	4683.822085	25.212455
167.591027	4681.619522	25.217472
167.548573	4682.555394	25.222490
167.943519	4696.214497	25.227507
168.080239	4719.882798	25.232525
168.257880	4702.390230	25.237543
168.425973	4731.236191	25.242560
168.586993	4741.379194	25.247578
168.745615	4736.766806	25.252595
168.836134	4748.304825	25.257613
169.361149	4754.908742	25.262631
169.622166	4763.099794	25.267648
169.602297	4771.495328	25.272666
170.107163	4758.370109	25.277683
170.305273	4768.710182	25.282701
170.276243	4766.467296	25.287719
170.688558	4772.213611	25.292736
170.588061	4788.763391	25.297754
170.825113	4784.232886	25.302771
170.444072	4788.206636	25.307789
170.896084	4796.326349	25.312807
170.970592	4797.799768	25.317824
171.043112	4819.448033	25.322842
171.442391	4806.946140	25.327859
171.354063	4822.220375	25.332877
171.458619	4829.655230	25.337895
172.080012	4834.905666	25.342912
171.950833	4847.101844	25.347930
172.126273	4834.176188	25.352947
172.283905	4847.007911	25.357965
172.401996	4858.455086	25.362983
173.029729	4863.912994	25.368000
172.685370	4879.722146	25.373018
173.119528	4869.546384	25.378035
172.933682	4865.849510	25.383053
173.655095	4889.967686	25.388071
173.440700	4887.844802	25.393088
173.610107	4884.063753	25.398106
173.732891	4879.819698	25.403123
173.879546	4901.929852	25.408141
173.980063	4913.036875	25.413159
174.479992	4909.870239	25.418176
174.389350	4918.839623	25.423194
174.848431	4918.722417	25.428211
174.932808	4935.895056	25.433229
174.576640	4945.070419	25.438247
175.186927	4932.845523	25.443264
175.086401	4969.049433	25.448282
175.578638	4962.833216	25.453299
175.830162	4965.811696	25.458317
176.184520	4976.034176	25.463335
176.483053	4977.667785	25.468352
176.441647	4988.045411	25.473370
176.614360	4989.068151	25.478387
176.728677	4990.302381	25.483405
176.801591	4995.422403	25.488423
176.955223	5003.289284	25.493440
177.470185	5015.367962	25.498458
177.469196	5008.641124	25.503475
177.461327	5018.468244	25.508493
177.855602	5024.610097	25.513511
177.891500	5028.197254	25.518528
177.501975	5033.959008	25.523546
177.940055	5050.966828	25.528563
178.199871	5058.551694	25.533581
178.433994	5080.549049	25.538599
178.755951	5066.315152	25.543616
178.757714	5108.135859	25.548634
179.530804	5072.395604	25.553651
179.148361	5116.459101	25.558669
179.601125	5102.644868	25.563687
179.656396	5101.398615	25.568704
179.596290	5131.526301	25.573722
180.059075	5120.919412	25.578739
180.581329	5119.516892	25.583757
180.483422	5140.715273	25.588775
181.003208	5149.183903	25.593792
181.067443	5150.293965	25.598810
181.214924	5141.742634	25.603827
181.187009	5143.937301	25.608845
181.469838	5149.766559	25.613863
181.472493	5147.327395	25.618880
181.134845	5154.161067	25.623898
181.760547	5161.535823	25.628915
182.008838	5163.300975	25.633933
181.891645	5169.582645	25.638951
182.033781	5171.584213	25.643968
182.355604	5193.120908	25.648986
182.568803	5194.114394	25.654003
182.862223	5197.387551	25.659021
182.720089	5231.650069	25.664039
183.069898	5205.882408	25.669056
183.083546	5248.086316	25.674074
183.506952	5206.439812	25.679092
183.892691	5264.775653	25.684109
183.886501	5242.635554	25.689127
184.267908	5267.078399	25.694144
184.468407	5243.181668	25.699162
184.289535	5265.673110	25.704180
184.640762	5265.963307	25.709197
184.496554	5284.974358	25.714215
185.186513	5278.383485	25.719232
184.944447	5277.697553	25.724250
185.348426	5304.727497	25.729268
185.536081	5300.293610	25.734285
185.433914	5298.517021	25.739303
185.772463	5302.081171	25.744320
185.901539	5343.492827	25.749338
185.992839	5318.311374	25.754356
186.541830	5342.641090	25.759373
186.572618	5344.164803	25.764391
187.318660	5351.927203	25.769408
187.079407	5355.555157	25.774426
187.704684	5348.904548	25.779444
187.736082	5381.382232	25.784461
187.401051	5373.192480	25.789479
187.996209	5361.910557	25.794496
187.945555	5403.459601	25.799514
188.258834	5372.985041	25.804532
188.181467	5392.479632	25.809549
188.365879	5411.355852	25.814567
188.993712	5387.355361	25.819584
188.661436	5404.411664	25.824602
188.916284	5425.688747	25.829620
189.315420	5428.198509	25.834637
189.334654	5411.672842	25.839655
189.465672	5425.627239	25.844672
189.905358	5461.107423	25.849690
189.960723	5460.951517	25.854708
190.475190	5433.399679	25.859725
190.253350	5494.008564	25.864743
191.069946	5477.051249	25.869760
190.856229	5493.474326	25.874778
191.135960	5481.960951	25.879796
191.454097	5466.205762	25.884813
191.302742	5496.035626	25.889831
191.657553	5470.079467	25.894848
191.332818	5522.291690	25.899866
191.986862	5492.929269	25.904884
192.059064	5511.402611	25.909901
191.943946	5521.883623	25.914919
192.369903	5505.838998	25.919936
192.203125	5541.869209	25.924954
192.058550	5538.129395	25.929972
192.978469	5541.198121	25.934989
192.569754	5575.968890	25.940007
193.362837	5566.458436	25.945024
193.389896	5580.992062	25.950042
193.414111	5592.476802	25.955060
193.585784	5601.241144	25.960077
194.055843	5625.055231	25.965095
194.491899	5605.980772	25.970112
194.400931	5628.912694	25.975130
194.580363	5635.731814	25.980148
194.955859	5628.718883	25.985165
194.868651	5658.213929	25.990183
195.250863	5631.217783	25.995200
195.295363	5676.953559	26.000218
195.708235	5657.454748	26.005236
196.244291	5673.246337	26.010253
196.359194	5676.071302	26.015271
196.525308	5667.515124	26.020288
196.579895	5695.517240	26.025306
196.567508	5693.797096	26.030324
196.967026	5714.155447	26.035341
196.671932	5700.594411	26.040359
196.841320	5701.792388	26.045376
196.928128	5722.662413	26.050394
197.328749	5729.089925	26.055412
197.496789	5742.141056	26.060429
197.342997	5769.523542	26.065447
198.301651	5750.745580	26.070464
198.587903	5774.744199	26.075482
198.457337	5786.551152	26.080500
198.800130	5780.059463	26.085517
199.164828	5810.270295	26.090535
199.533020	5811.892111	26.095552
199.302825	5799.309568	26.100570
199.690072	5823.560445	26.105588
200.362853	5834.536813	26.110605
199.939116	5824.593143	26.115623
200.029924	5851.670084	26.120640
200.688588	5823.956068	26.125658
200.673844	5868.723180	26.130676
200.840407	5842.328268	26.135693
200.719948	5867.021265	26.140711
201.211626	5859.345364	26.145728
201.295864	5874.306018	26.150746
201.542580	5885.873528	26.155764
201.966951	5898.028747	26.160781
201.444093	5891.119567	26.165799
201.976958	5919.138699	26.170816
202.470174	5909.140847	26.175834
202.362356	5917.130932	26.180852
202.577092	5915.846602	26.185869
202.792897	5939.918086	26.190887
203.024849	5935.846720	26.195904
203.013850	5944.285565	26.200922
203.234133	5966.478418	26.205940
203.587704	5979.234263	26.210957
203.381755	5977.725894	26.215975
203.559930	5999.956980	26.220992
204.230394	5997.309727	26.226010
204.290355	6009.817374	26.231028
204.857326	6018.061848	26.236045
204.751875	6037.177045	26.241063
205.606628	6031.212581	26.246080
205.569400	6031.569443	26.251098
205.803254	6030.754893	26.256116
206.049792	6058.545359	26.261133
206.068804	6038.679268	26.266151
206.255052	6057.268860	26.271168
206.578857	6057.505230	26.276186
206.681837	6053.884744	26.281204
207.012333	6089.355526	26.286221
207.245479	6081.033891	26.291239
207.098492	6066.208199	26.296256
207.362960	6077.872162	26.301274
207.252669	6101.865293	26.306292
208.130932	6100.770994	26.311309
207.895164	6112.550131	26.316327
207.961138	6111.045606	26.321344
208.480309	6127.973303	26.326362
208.300627	6135.704318	26.331380
208.790533	6144.246742	26.336397
208.977808	6162.512946	26.341415
208.948078	6150.281298	26.346432
209.203967	6171.271341	26.351450
209.122654	6190.596886	26.356468
209.814087	6185.651286	26.361485
209.642720	6212.664469	26.366503
209.840868	6224.268312	26.371520
210.177568	6230.731412	26.376538
210.450632	6252.681040	26.381556
210.791085	6247.329541	26.386573
211.161016	6264.761111	26.391591
211.326063	6282.374847	26.396608
211.567465	6282.403278	26.401626
211.639226	6291.753575	26.406644
212.113699	6295.495356	26.411661
212.017107	6296.274739	26.416679
212.182672	6308.200908	26.421696
212.636347	6322.609036	26.426714
212.811228	6332.684840	26.431732
213.285847	6321.494581	26.436749
212.908738	6352.430585	26.441767
213.489368	6346.169813	26.446784
213.872978	6363.734644	26.451802
213.916013	6373.691450	26.456820
214.189434	6352.191964	26.461837
214.102616	6374.948931	26.466855
214.279039	6381.465185	26.471872
214.598346	6383.642451	26.476890
214.505188	6382.894173	26.481908
214.876561	6411.647292	26.486925
214.833923	6427.553973	26.491943
215.006759	6417.432190	26.496960
215.176830	6449.516401	26.501978
215.349811	6457.569803	26.506996
216.296335	6452.467799	26.512013
216.495400	6476.186418	26.517031
216.375122	6492.002477	26.522048
216.672069	6488.823818	26.527066
216.802085	6498.209018	26.532084
216.709720	6524.464314	26.537101
216.961328	6513.949110	26.542119
216.961363	6551.041722	26.547136
217.536736	6525.794424	26.552154
217.695452	6591.031604	26.557172
218.300438	6540.541264	26.562189
218.677912	6585.820797	26.567207
218.796597	6574.361360	26.572224
219.581589	6587.166194	26.577242
219.586361	6580.292167	26.582260
219.550112	6590.195667	26.587277
219.697336	6587.003088	26.592295
219.955465	6589.917122	26.597312
220.236221	6595.340525	26.602330
220.018626	6612.663173	26.607348
220.258530	6622.343288	26.612365
220.432012	6629.649262	26.617383
220.516182	6634.922270	26.622400
220.733772	6660.018247	26.627418
220.866898	6679.414889	26.632436
221.494733	6667.909625	26.637453
221.472816	6675.720413	26.642471
221.734363	6710.251668	26.647488
222.126380	6712.665232	26.652506
222.505437	6708.962027	26.657524
222.897889	6734.020815	26.662541
223.117114	6727.212457	26.667559
223.302084	6744.098938	26.672576
223.400444	6741.365731	26.677594
223.453016	6750.367683	26.682612
223.771207	6755.498001	26.687629
223.937222	6776.576402	26.692647
224.027611	6785.922468	26.697664
224.523249	6783.417826	26.702682
224.476222	6808.424055	26.707700
224.767228	6804.464207	26.712717
224.804626	6808.250616	26.717735
225.143519	6827.395924	26.722752
225.512065	6840.857457	26.727770
225.241985	6830.991679	26.732788
225.535097	6849.597493	26.737805
226.434731	6856.785469	26.742823
226.526843	6843.899669	26.747840
227.067626	6852.726299	26.752858
226.672415	6865.654988	26.757876
227.028002	6879.135932	26.762893
227.272747	6885.180456	26.767911
227.107391	6889.563338	26.772928
227.453807	6899.771907	26.777946
227.800627	6919.182008	26.782964
227.841571	6926.181948	26.787981
228.069111	6946.033607	26.792999
228.083532	6945.390105	26.798016
228.543930	6955.830746	26.803034
228.793658	6984.991477	26.808052
229.003569	6989.857462	26.813069
229.305896	6999.420870	26.818087
229.639025	7016.278537	26.823104
229.688120	7021.967984	26.828122
230.154883	7037.491987	26.833140
230.130544	7046.517394	26.838157
230.773585	7052.514235	26.843175
230.752384	7071.502461	26.848192
231.256225	7054.154970	26.853210
231.180125	7081.509397	26.858228
231.453071	7096.349937	26.863245
231.926500	7101.782942	26.868263
231.844937	7088.354967	26.873280
232.184580	7127.242308	26.878298
232.583598	7106.831111	26.883316
233.084891	7117.886140	26.888333
233.265175	7151.707515	26.893351
233.167896	7144.918733	26.898368
233.823616	7130.500625	26.903386
233.465191	7147.759795	26.908404
233.768848	7155.323024	26.913421
234.209643	7164.834569	26.918439
234.327354	7174.495971	26.923456
234.755775	7185.587844	26.928474
234.860128	7197.091742	26.933492
234.993524	7197.705473	26.938509
235.165496	7215.916408	26.943527
235.093189	7233.839775	26.948544
235.617631	7250.310787	26.953562
235.987796	7260.139724	26.958580
235.812990	7269.012216	26.963597
236.415773	7272.270366	26.968615
236.424529	7287.569436	26.973632
236.623546	7291.788921	26.978650
236.899257	7323.308987	26.983668
237.383336	7315.089868	26.988685
237.696942	7319.859178	26.993703
237.694375	7341.276834	26.998720
237.959303	7341.303096	27.003738
238.235179	7356.634406	27.008756
238.145467	7360.451446	27.013773
238.783440	7380.320095	27.018791
238.954836	7361.387864	27.023808
239.482032	7383.522122	27.028826
239.597241	7410.474493	27.033844
239.806487	7394.296363	27.038861
239.849774	7403.886374	27.043879
240.072488	7422.497836	27.048896
240.661293	7407.714815	27.053914
240.750674	7425.965137	27.058932
240.781182	7430.385410	27.063949
241.157772	7432.957348	27.068967
241.030550	7449.449053	27.073984
241.650401	7457.546648	27.079002
241.491865	7467.514287	27.084020
241.854840	7475.997467	27.089037
242.320588	7489.448034	27.094055
241.904739	7500.458341	27.099072
242.232567	7509.454647	27.104090
242.359352	7527.456789	27.109108
242.547586	7539.441711	27.114125
243.095050	7572.594938	27.119143
243.484719	7581.116413	27.124160
243.720705	7595.574651	27.129178
244.030908	7610.430226	27.134196
243.937039	7630.354491	27.139213
244.755665	7635.363649	27.144231
244.880254	7655.469506	27.149248
245.356386	7654.430563	27.154266
245.834933	7660.774119	27.159284
245.880629	7666.716930	27.164301
246.708658	7680.804703	27.169319
246.625412	7684.629450	27.174336
246.834895	7684.054753	27.179354
246.631972	7690.121394	27.184372
247.042367	7704.056230	27.189389
247.290951	7708.024014	27.194407
247.181084	7721.516971	27.199424
247.374825	7732.528638	27.204442
247.911736	7735.090812	27.209460
247.770554	7750.646375	27.214477
248.408930	7755.258625	27.219495
248.476547	7779.507403	27.224512
248.507348	7787.168740	27.229530
248.762677	7798.092741	27.234548
249.282479	7816.773796	27.239565
249.410739	7822.738918	27.244583
249.890279	7846.001931	27.249600
250.411237	7849.444003	27.254618
250.466973	7857.350832	27.259636
250.479760	7870.226370	27.264653
250.606312	7880.007997	27.269671
251.096906	7893.889313	27.274688
251.354796	7887.447232	27.279706
251.654047	7894.393081	27.284724
251.737420	7899.680043	27.289741
252.103914	7904.103557	27.294759
252.373265	7914.646934	27.299776
252.423233	7936.201067	27.304794
253.076500	7935.460416	27.309812
252.637777	7941.822043	27.314829
253.476242	7941.389433	27.319847
253.596240	7963.560350	27.324864
253.340200	7964.224385	27.329882
253.764904	7983.499145	27.334900
253.922756	7992.476415	27.339917
254.375799	8001.936979	27.344935
254.406554	8023.163033	27.349952
254.378978	8032.180898	27.354970
254.663025	8054.812867	27.359988
254.825318	8077.917507	27.365005
255.391747	8092.229923	27.370023
255.570116	8115.513036	27.375040
256.029881	8116.023641	27.380058
256.496443	8133.227203	27.385076
256.374167	8148.337164	27.390093
257.223273	8161.260630	27.395111
257.103221	8171.773408	27.400128
257.644540	8175.078546	27.405146
257.933243	8191.894274	27.410164
257.944175	8197.768874	27.415181
258.469085	8208.767452	27.420199
258.753585	8229.500909	27.425216
259.036250	8235.840527	27.430234
259.293518	8237.725809	27.435252
259.337329	8247.760074	27.440269
259.882366	8251.580035	27.445287
259.927906	8274.942798	27.450304
259.908622	8283.662844	27.455322
260.450879	8299.058898	27.460340
260.724130	8317.215697	27.465357
260.929344	8314.556450	27.470375
261.134001	8334.823576	27.475392
261.157249	8342.892429	27.480410
261.697303	8351.820800	27.485428
261.320510	8372.260913	27.490445
261.944066	8378.575374	27.495463
262.302512	8411.184611	27.500480
262.695012	8425.321271	27.505498
262.919057	8429.711781	27.510516
263.074961	8449.018973	27.515533
263.489705	8456.445559	27.520551
263.561594	8461.969828	27.525568
263.617416	8473.436023	27.530586
264.299852	8500.967234	27.535604
264.411254	8509.189732	27.540621
264.696895	8522.080572	27.545639
265.312634	8529.223357	27.550656
265.078465	8535.971250	27.555674
265.748581	8535.562317	27.560692
265.716917	8551.997517	27.565709
266.122984	8551.729030	27.570727
266.328611	8572.993306	27.575744
266.661581	8573.067748	27.580762
266.975645	8596.880805	27.585780
266.636173	8618.411830	27.590797
267.354185	8605.558127	27.595815
267.326818	8626.523615	27.600832
267.249174	8653.738352	27.605850
268.135630	8653.119853	27.610868
267.687217	8691.262657	27.615885
268.292567	8698.219113	27.620903
268.793361	8707.790553	27.625920
269.248607	8721.355262	27.630938
269.478397	8737.914241	27.635956
269.456047	8752.504485	27.640973
269.984654	8762.881636	27.645991
270.259272	8764.277133	27.651008
270.172117	8794.858404	27.656026
271.020997	8797.223112	27.661044
271.329614	8797.407669	27.666061
271.349022	8828.474064	27.671079
271.171541	8856.051710	27.676096
271.521903	8851.876881	27.681114
272.101277	8854.051239	27.686132
272.008886	8872.934677	27.691149
273.061791	8893.762985	27.696167
273.261845	8896.498276	27.701184
273.521140	8913.758599	27.706202
273.701533	8920.520067	27.711220
273.918214	8931.190598	27.716237
274.120213	8935.887336	27.721255
274.388861	8953.702556	27.726272
274.759025	8962.479355	27.731290
274.793516	8979.282194	27.736308
274.982807	8979.926047	27.741325
275.089022	9026.694716	27.746343
275.690802	9007.214547	27.751360
275.642823	9055.728456	27.756378
276.018671	9043.628874	27.761396
276.595647	9076.459695	27.766413
276.468090	9079.914536	27.771431
276.957072	9108.658466	27.776448
276.997578	9122.483224	27.781466
277.439463	9110.942002	27.786484
277.379177	9162.151425	27.791501
278.520636	9165.432357	27.796519
278.420191	9179.336684	27.801536
278.921368	9181.027011	27.806554
279.052301	9205.074039	27.811572
279.656028	9223.159598	27.816589
279.843412	9209.526313	27.821607
280.151143	9228.263408	27.826624
280.524236	9225.265233	27.831642
280.336629	9244.856017	27.836660
280.391926	9260.810704	27.841677
280.536853	9255.069486	27.846695
281.241350	9297.164558	27.851712
281.346183	9290.824966	27.856730
281.425923	9299.193411	27.861748
281.589105	9322.232554	27.866765
281.985483	9315.862617	27.871783
281.962313	9362.368090	27.876800
282.759945	9361.519391	27.881818
283.117075	9383.946179	27.886836
283.696570	9400.740141	27.891853
283.680528	9392.273819	27.896871
284.142087	9419.668024	27.901888
283.927141	9423.005847	27.906906
284.072478	9433.825822	27.911924
284.318178	9471.719119	27.916941
284.780606	9475.714680	27.921959
285.268162	9487.037692	27.926976
285.422827	9532.806717	27.931994
285.323189	9527.074077	27.937012
286.095336	9547.693874	27.942029
285.683221	9581.055665	27.947047
286.957824	9569.219661	27.952064
287.112912	9620.486822	27.957082
287.644529	9608.009807	27.962100
287.694602	9615.934210	27.967117
288.292176	9639.724206	27.972135
288.208438	9660.206713	27.977152
288.646060	9653.953218	27.982170
288.912341	9670.494825	27.987188
289.459371	9678.848422	27.992205
289.728187	9680.509347	27.997223
290.038980	9710.595850	28.002240
290.009105	9700.999933	28.007258
290.656276	9736.779928	28.012276
290.590185	9745.247412	28.017293
290.899684	9741.713920	28.022311
291.410159	9758.839181	28.027328
291.393395	9769.870953	28.032346
292.030439	9785.420277	28.037364
292.315771	9805.011569	28.042381
292.217597	9786.009852	28.047399
292.556829	9834.370527	28.052416
292.856206	9831.454810	28.057434
292.972634	9839.463976	28.062452
293.345386	9860.354436	28.067469
293.819468	9889.688918	28.072487
294.062386	9880.291004	28.077504
293.913481	9903.794324	28.082522
294.751780	9911.385897	28.087540
294.743124	9950.625715	28.092557
295.492404	9949.532478	28.097575
295.592963	9942.322526	28.102592
295.578699	9974.107283	28.107610
295.913421	9981.459251	28.112628
296.217513	9989.818690	28.117645
296.708662	9998.219542	28.122663
296.957703	10004.095069	28.127680
296.905236	10033.636124	28.132698
297.400683	10042.890168	28.137716
297.708174	10062.058028	28.142733
297.969119	10073.214960	28.147751
298.357263	10086.758164	28.152768
298.453317	10097.422784	28.157786
298.783233	10120.657326	28.162804
298.866547	10137.125517	28.167821
298.818069	10150.804863	28.172839
299.226671	10181.213544	28.177856
299.877475	10199.290820	28.182874
300.196547	10208.281899	28.187892
300.438791	10236.738369	28.192909
300.433978	10255.431338	28.197927
301.186959	10259.826235	28.202944
301.663338	10294.315424	28.207962
301.695004	10292.097442	28.212980
301.885970	10339.348556	28.217997
302.265840	10328.633567	28.223015
302.987581	10366.879014	28.228032
302.896968	10354.813377	28.233050
303.365980	10379.613486	28.238068
303.870822	10384.489463	28.243085
303.959558	10395.203466	28.248103
304.383468	10428.214326	28.253120
304.851923	10425.640646	28.258138
304.808694	10447.318308	28.263156
305.171496	10464.929479	28.268173
305.018634	10483.365767	28.273191
306.298195	10480.261056	28.278208
306.139527	10518.537416	28.283226
306.700217	10508.760690	28.288244
307.377320	10533.682928	28.293261
307.097455	10551.874718	28.298279
307.823759	10530.478858	28.303296
308.391905	10547.459685	28.308314
308.323250	10597.841915	28.313332
308.377302	10588.707005	28.318349
308.581451	10591.456911	28.323367
308.796868	10640.951934	28.328384
308.837543	10639.812219	28.333402
309.670464	10623.791713	28.338420
309.845496	10676.798946	28.343437
309.906163	10712.866378	28.348455
310.405148	10691.066589	28.353472
310.728024	10745.878694	28.358490
311.063081	10717.193180	28.363508
311.395436	10745.375364	28.368525
311.317466	10786.551438	28.373543
312.114278	10756.540143	28.378560
311.998317	10806.189649	28.383578
312.482750	10808.904372	28.388596
312.996654	10822.194461	28.393613
313.345338	10837.915581	28.398631
313.801344	10839.525953	28.403648
313.702543	10869.309770	28.408666
314.328582	10873.477965	28.413684
314.285771	10858.927207	28.418701
314.351871	10928.494344	28.423719
314.747621	10892.545369	28.428736
315.276091	10907.099112	28.433754
314.997401	10957.849314	28.438772
315.573747	10969.819213	28.443789
315.912185	10997.392148	28.448807
316.319711	10979.199228	28.453824
316.473454	11047.296582	28.458842
316.717663	11032.325690	28.463860
316.834732	11081.126175	28.468877
317.421543	11089.525386	28.473895
317.758136	11100.266501	28.478912
318.288512	11127.905496	28.483930
318.663301	11137.232576	28.488948
319.179785	11181.016433	28.493965
319.229474	11179.725314	28.498983
319.878028	11209.960111	28.504000
319.904238	11208.651481	28.509018
319.968377	11251.741071	28.514036
320.806733	11253.369260	28.519053
320.811162	11266.652003	28.524071
321.258890	11289.437501	28.529088
321.678957	11323.453218	28.534106
321.989879	11317.876406	28.539124
322.507506	11367.314240	28.544141
322.482051	11343.644468	28.549159
323.086993	11382.297155	28.554176
323.172337	11371.170711	28.559194
323.590592	11396.895907	28.564212
324.001057	11427.061653	28.569229
324.435938	11437.417835	28.574247
324.755794	11457.590549	28.579264
325.320242	11448.378897	28.584282
325.229223	11509.319514	28.589300
325.565561	11484.884317	28.594317
325.981535	11523.896463	28.599335
325.699043	11532.508833	28.604352
326.377968	11543.778908	28.609370
326.529184	11573.997675	28.614388
327.171513	11597.766338	28.619405
327.027536	11603.930615	28.624423
327.593043	11643.452856	28.629440
328.125970	11652.561836	28.634458
328.138768	11677.713832	28.639476
328.904339	11686.601197	28.644493
329.004151	11710.018501	28.649511
329.462245	11733.100130	28.654528
329.390013	11744.705320	28.659546
329.853607	11758.228174	28.664564
329.835903	11776.817256	28.669581
330.504013	11771.367134	28.674599
330.948389	11821.378511	28.679616
331.500718	11825.661437	28.684634
331.649641	11839.725239	28.689652
332.416799	11867.106303	28.694669
332.718676	11849.495859	28.699687
332.629247	11876.109117	28.704704
333.428027	11866.633593	28.709722
333.269694	11930.135120	28.714740
333.854733	11903.283877	28.719757
334.385459	11939.089256	28.724775
334.485661	11936.146641	28.729792
334.868040	11948.776703	28.734810
334.913296	11988.580504	28.739828
335.169283	11969.316335	28.744845
335.439561	12011.869160	28.749863
335.646970	12034.295435	28.754880
336.618740	12011.920396	28.759898
336.718308	12056.585484	28.764916
337.022123	12093.745529	28.769933
337.136469	12082.877806	28.774951
337.694866	12068.186591	28.779968
337.882900	12140.843281	28.784986
338.214218	12155.977063	28.790004
338.831823	12162.057983	28.795021
339.039913	12169.958549	28.800039
339.055292	12218.209265	28.805056
339.683875	12208.890521	28.810074
339.693265	12263.760454	28.815092
340.331688	12237.083505	28.820109
340.291283	12306.025006	28.825127
340.856853	12297.670190	28.830144
341.011874	12338.110889	28.835162
341.496007	12347.584421	28.840180
341.839920	12351.014262	28.845197
342.176875	12394.449695	28.850215
342.589738	12398.981300	28.855232
342.435805	12428.798810	28.860250
343.117941	12430.430197	28.865268
343.650995	12478.727149	28.870285
344.110007	12474.720173	28.875303
344.473804	12525.370486	28.880320
345.282614	12510.628907	28.885338
345.229059	12573.715998	28.890356
345.507680	12566.835141	28.895373
345.892648	12589.096989	28.900391
346.056517	12602.638850	28.905408
346.386485	12606.348227	28.910426
346.598392	12648.994788	28.915444
347.255309	12652.044240	28.920461
347.360264	12688.563284	28.925479
347.839355	12702.029421	28.930496
348.849640	12702.458006	28.935514
348.550429	12742.464486	28.940532
349.093473	12719.192338	28.945549
349.047167	12767.611656	28.950567
349.776934	12751.144126	28.955584
349.626594	12795.147149	28.960602
349.855539	12796.029648	28.965620
350.196784	12830.543815	28.970637
350.657016	12859.096628	28.975655
350.937292	12866.912855	28.980672
351.472626	12909.351975	28.985690
351.453042	12897.642339	28.990708
352.254893	12929.112582	28.995725
352.190894	12935.593469	29.000743
352.954733	12980.468498	29.005760
353.299669	12982.396508	29.010778
353.826180	13011.211389	29.015796
354.217717	13014.964974	29.020813
354.034739	13054.397654	29.025831
354.979473	13058.461970	29.030848
354.995319	13067.956071	29.035866
355.299284	13112.326633	29.040884
355.848477	13117.837361	29.045901
356.341658	13137.013588	29.050919
356.507031	13174.079093	29.055936
357.177191	13160.821858	29.060954
357.370584	13194.721269	29.065972
357.861292	13220.107826	29.070989
358.016796	13223.023004	29.076007
358.077243	13269.293006	29.081024
358.605058	13277.748113	29.086042
358.840125	13295.159994	29.091060
359.212954	13312.551912	29.096077
359.600587	13350.482711	29.101095
359.887747	13363.859789	29.106112
360.589397	13385.173634	29.111130
360.676038	13397.898477	29.116148
361.598416	13413.810694	29.121165
361.721315	13448.945706	29.126183
362.002268	13461.911398	29.131200
362.397268	13475.189725	29.136218
362.650787	13503.943762	29.141236
363.263899	13517.011444	29.146253
363.422777	13532.013505	29.151271
363.804393	13545.932989	29.156288
364.352657	13568.866780	29.161306
364.664478	13581.726607	29.166324
365.418753	13601.922990	29.171341
365.673892	13627.003193	29.176359
365.735560	13639.509946	29.181376
365.826129	13648.744845	29.186394
366.188847	13675.347157	29.191412
366.532305	13705.351801	29.196429
367.280105	13714.503070	29.201447
367.455909	13734.560481	29.206464
367.755189	13739.423390	29.211482
368.022763	13772.681265	29.216500
368.301022	13761.512691	29.221517
368.579721	13791.421853	29.226535
368.569013	13815.369011	29.231552
369.374487	13837.832239	29.236570
369.651109	13862.298965	29.241588
370.127073	13872.036688	29.246605
370.537096	13901.881257	29.251623
370.880818	13922.909593	29.256640
371.065427	13932.090321	29.261658
371.235748	13959.235763	29.266676
371.841098	13977.989201	29.271693
372.157565	14020.672440	29.276711
372.517400	14044.305871	29.281728
372.897349	14041.147560	29.286746
373.014054	14094.282205	29.291764
373.713064	14101.290833	29.296781
374.000271	14122.012203	29.301799
373.982570	14165.149173	29.306816
374.438575	14179.369502	29.311834
374.886252	14231.994538	29.316852
375.695054	14244.566544	29.321869
376.174708	14257.343819	29.326887
376.099581	14311.363285	29.331904
376.843587	14314.069481	29.336922
377.207491	14341.381232	29.341940
377.463481	14362.754968	29.346957
377.816777	14376.674219	29.351975
378.154530	14400.637124	29.356992
378.980807	14424.826770	29.362010
378.843819	14449.785818	29.367028
379.635044	14469.381568	29.372045
380.180064	14498.563546	29.377063
380.118187	14520.227360	29.382080
380.955558	14521.488978	29.387098
381.204414	14549.999537	29.392116
381.808025	14565.321709	29.397133
382.195499	14582.729672	29.402151
382.362666	14607.312154	29.407168
382.839691	14620.426583	29.412186
382.912094	14653.521366	29.417204
383.390927	14663.900317	29.422221
383.779960	14686.320360	29.427239
384.271206	14704.911723	29.432256
384.668786	14725.438222	29.437274
384.697727	14748.254426	29.442292
385.367432	14765.377309	29.447309
385.511519	14793.009469	29.452327
386.002858	14816.381471	29.457344
386.265680	14836.027153	29.462362
386.405670	14866.185370	29.467380
386.702344	14900.850864	29.472397
387.405071	14931.811557	29.477415
387.615941	14965.094645	29.482432
387.873349	14967.162327	29.487450
387.991343	14991.353846	29.492468
388.784378	15020.573961	29.497485
389.530911	15050.263836	29.502503
389.565499	15054.700947	29.507520
390.098836	15084.461170	29.512538
390.199603	15115.111154	29.517556
390.466650	15132.051837	29.522573
391.268539	15140.512343	29.527591
391.600944	15187.370467	29.532608
391.993463	15215.602444	29.537626
392.206220	15226.391025	29.542644
392.474430	15255.084715	29.547661
393.074821	15283.963275	29.552679
392.916320	15325.533176	29.557696
394.153283	15333.037747	29.562714
393.996393	15377.078172	29.567732
394.591966	15385.023476	29.572749
395.289614	15401.643342	29.577767
395.656302	15456.748177	29.582784
396.007330	15469.269169	29.587802
396.626308	15489.660160	29.592820
396.562043	15500.196970	29.597837
396.943976	15535.894203	29.602855
397.414344	15561.636164	29.607872
397.997323	15571.494813	29.612890
398.213688	15600.165427	29.617908
398.392876	15643.410493	29.622925
399.194763	15659.319283	29.627943
399.645077	15690.897116	29.632960
399.972246	15717.478931	29.637978
400.451489	15749.441080	29.642996
400.769810	15780.835244	29.648013
400.971749	15789.615484	29.653031
401.006300	15827.273221	29.658048
401.814475	15859.470147	29.663066
401.823871	15892.258109	29.668084
402.333666	15909.870006	29.673101
403.209793	15941.056057	29.678119
403.421977	15985.900885	29.683136
404.172678	15987.302220	29.688154
404.425317	16022.436735	29.693172
404.949456	16047.806932	29.698189
405.269380	16082.932538	29.703207
405.447348	16082.602301	29.708224
406.371764	16125.397167	29.713242
406.980658	16130.442483	29.718260
407.066068	16152.452001	29.723277
408.130283	16163.989891	29.728295
407.850711	16213.349259	29.733312
408.609561	16206.128302	29.738330
409.012766	16225.619168	29.743348
409.158180	16262.339876	29.748365
409.396168	16259.508518	29.753383
409.516254	16285.477656	29.758400
410.231969	16299.412166	29.763418
410.518251	16329.035063	29.768436
410.883665	16354.211206	29.773453
411.291308	16362.076057	29.778471
411.612724	16383.912891	29.783488
411.701905	16416.180962	29.788506
412.260534	16434.785051	29.793524
412.495010	16454.477279	29.798541
412.702666	16507.437995	29.803559
413.154880	16511.648085	29.808576
413.796394	16556.976887	29.813594
414.447588	16583.959404	29.818612
414.613363	16611.949109	29.823629
415.478431	16632.998785	29.828647
415.460250	16653.533586	29.833664
416.061042	16675.832165	29.838682
416.229221	16713.692698	29.843700
416.788732	16739.588064	29.848717
417.624011	16761.579756	29.853735
417.984189	16789.808070	29.858752
418.187621	16802.509851	29.863770
418.200735	16821.072203	29.868788
418.658553	16862.267081	29.873805
419.440528	16892.573419	29.878823
419.492751	16936.630447	29.883840
420.033521	16951.638393	29.888858
420.615498	16977.913414	29.893876
420.919303	17030.153788	29.898893
421.933670	17030.184912	29.903911
422.095009	17068.597153	29.908928
422.743105	17088.056396	29.913946
423.084283	17104.562291	29.918964
423.656324	17149.597046	29.923981
423.992511	17156.471423	29.928999
423.908691	17199.073648	29.934016
424.470511	17185.902089	29.939034
425.142628	17251.282947	29.944052
425.299392	17252.413421	29.949069
425.847486	17288.299646	29.954087
425.959400	17337.733289	29.959104
426.569168	17336.680744	29.964122
427.228464	17382.197709	29.969140
427.334306	17412.581299	29.974157
427.879880	17444.929976	29.979175
428.434421	17472.292416	29.984192
428.589137	17486.359707	29.989210
429.351206	17529.723484	29.994228
429.772385	17560.163023	29.999245
430.180323	17566.446467	30.004263
430.096646	17605.143351	30.009280
430.790667	17614.044453	30.014298
431.415591	17672.365767	30.019316
431.780297	17674.141844	30.024333
432.389647	17724.130109	30.029351
432.221017	17734.306842	30.034368
432.840722	17745.268566	30.039386
433.283280	17807.211766	30.044404
433.386275	17811.208972	30.049421
434.692045	17801.045184	30.054439
434.534516	17886.529979	30.059456
434.676439	17888.052217	30.064474
435.430273	17898.497823	30.069492
435.681629	17949.191459	30.074509
436.325990	17990.386003	30.079527
436.569697	17997.391431	30.084544
437.176458	18010.799802	30.089562
437.594678	18085.075093	30.094580
438.025281	18075.481253	30.099597
438.656831	18110.307898	30.104615
438.793074	18176.953989	30.109632
439.395077	18173.017670	30.114650
439.705914	18219.594557	30.119668
439.771017	18230.643803	30.124685
440.851245	18274.843610	30.129703
440.967462	18299.357327	30.134720
441.876012	18322.366531	30.139738
441.843484	18376.921684	30.144756
442.142489	18386.153094	30.149773
443.166592	18431.885105	30.154791
443.393220	18451.274439	30.159808
443.810700	18465.279499	30.164826
444.212064	18527.046311	30.169844
444.589504	18536.610983	30.174861
445.543025	18587.348776	30.179879
445.742057	18595.729309	30.184896
446.595449	18607.767808	30.189914
446.734976	18666.996967	30.194932
447.059667	18696.298200	30.199949
447.786294	18692.793086	30.204967
448.509818	18716.109916	30.209984
449.306610	18720.562581	30.215002
449.871048	18779.760698	30.220020
450.090159	18783.530600	30.225037
450.770963	18780.680020	30.230055
451.049855	18805.673351	30.235072
451.378026	18819.890994	30.240090
451.444394	18851.147481	30.245108
451.596281	18847.431135	30.250125
452.301292	18904.973450	30.255143
452.438805	18905.837819	30.260160
452.852692	18948.674810	30.265178
453.376245	18976.472024	30.270196
453.720354	19008.322391	30.275213
453.915173	19055.050189	30.280231
454.457004	19056.389148	30.285248
454.733015	19125.076544	30.290266
455.386958	19126.103938	30.295284
455.467189	19192.877086	30.300301
456.515379	19197.363863	30.305319
456.554325	19237.002591	30.310336
456.962059	19274.440449	30.315354
457.640022	19293.151820	30.320372
457.917400	19324.150039	30.325389
458.230284	19340.668735	30.330407
458.774914	19402.912681	30.335424
459.232619	19435.912423	30.340442
459.573248	19449.715250	30.345460
460.308737	19473.436456	30.350477
460.630376	19520.931318	30.355495
461.028869	19525.702807	30.360512
461.557257	19612.575686	30.365530
462.447036	19612.648165	30.370548
462.644290	19638.507469	30.375565
462.999583	19684.168998	30.380583
463.840593	19696.713904	30.385600
464.102336	19737.907105	30.390618
464.616491	19754.214242	30.395636
464.677912	19796.666767	30.400653
465.338445	19829.562191	30.405671
466.177646	19868.216308	30.410688
466.432416	19900.324088	30.415706
467.202712	19911.916181	30.420724
467.288275	19960.797740	30.425741
468.125159	19979.637000	30.430759
468.387105	20005.792539	30.435776
468.938188	20047.271203	30.440794
469.854133	20072.898617	30.445812
469.633571	20103.936759	30.450829
470.277450	20139.989340	30.455847
470.660263	20175.935546	30.460864
470.863015	20204.546372	30.465882
471.477427	20220.128898	30.470900
472.158915	20266.794608	30.475917
472.156679	20291.427975	30.480935
472.978418	20323.432131	30.485952
473.528922	20358.447220	30.490970
473.936653	20413.180325	30.495988
474.037373	20451.394014	30.501005
474.892214	20460.297142	30.506023
475.317300	20509.632294	30.511040
475.445794	20547.546875	30.516058
476.529704	20571.891111	30.521076
476.995926	20592.086388	30.526093
477.358541	20641.465770	30.531111
477.925905	20679.228464	30.536128
478.760791	20679.082512	30.541146
479.482230	20704.600595	30.546164
480.027538	20727.870875	30.551181
480.257782	20741.884585	30.556199
481.050265	20775.287436	30.561216
481.719427	20798.926336	30.566234
482.487118	20813.377799	30.571252
482.649518	20820.823108	30.576269
482.991590	20839.909189	30.581287
483.512908	20854.080993	30.586304
483.649505	20864.986445	30.591322
484.302635	20888.359099	30.596340
484.036392	20913.615111	30.601357
484.695523	20927.898907	30.606375
485.298158	20944.222731	30.611392
485.402715	20980.327332	30.616410
486.101718	21003.028181	30.621428
486.187582	21036.733945	30.626445
486.790797	21062.021407	30.631463
487.295785	21099.730476	30.636480
486.986920	21140.398872	30.641498
488.159914	21152.810966	30.646516
488.108181	21194.682053	30.651533
488.597979	21251.728629	30.656551
489.507201	21286.529965	30.661568
489.750331	21317.916398	30.666586
490.151955	21361.094691	30.671604
490.786633	21408.791128	30.676621
491.413442	21442.606117	30.681639
491.878512	21473.233752	30.686656
492.310000	21522.791585	30.691674
493.189105	21554.108686	30.696692
493.464014	21579.140559	30.701709
493.858440	21616.039188	30.706727
494.541067	21650.105625	30.711744
494.568502	21696.152866	30.716762
495.215267	21737.860578	30.721780
495.815113	21773.234429	30.726797
496.318695	21814.361093	30.731815
496.865182	21850.704445	30.736832
497.399307	21905.782145	30.741850
498.103834	21930.048358	30.746868
498.735885	21967.039120	30.751885
499.064776	22029.516886	30.756903
500.109371	22042.452621	30.761920
499.913219	22063.472787	30.766938
500.359018	22112.286724	30.771956
500.712927	22160.217608	30.776973
501.398216	22185.392211	30.781991
501.893984	22212.582540	30.787008
502.302721	22277.001774	30.792026
503.075027	22305.544605	30.797044
503.565110	22341.358577	30.802061
503.731284	22400.894519	30.807079
504.697040	22415.349788	30.812096
505.290773	22476.034740	30.817114
505.850280	22489.024488	30.822132
506.396281	22534.771834	30.827149
506.755919	22558.072438	30.832167
507.258075	22608.802255	30.837184
507.525212	22643.201661	30.842202
508.172808	22666.545557	30.847220
508.714835	22712.184572	30.852237
509.039935	22738.660280	30.857255
509.558324	22759.892837	30.862272
510.134850	22811.040706	30.867290
510.544379	22842.346173	30.872308
511.044181	22862.251547	30.877325
511.619757	22893.953618	30.882343
512.231392	22939.857083	30.887360
512.577050	22967.156900	30.892378
513.246808	22996.296221	30.897396
513.875812	23030.646706	30.902413
513.999847	23066.782122	30.907431
514.688087	23103.575998	30.912448
515.146536	23129.618404	30.917466
515.586113	23186.716999	30.922484
516.017863	23213.883021	30.927501
516.251489	23251.147407	30.932519
517.244404	23277.452273	30.937536
517.278170	23338.506977	30.942554
518.181626	23368.841630	30.947572
519.236980	23385.382591	30.952589
519.336846	23440.937299	30.957607
519.950677	23473.740293	30.962624
520.302907	23491.114843	30.967642
521.123664	23533.692785	30.972660
521.525858	23581.084683	30.977677
521.984131	23612.350830	30.982695
522.616364	23628.353737	30.987712
523.421831	23669.536394	30.992730
523.766279	23708.550916	30.997748
524.543634	23730.873821	31.002765
524.704579	23783.632476	31.007783
525.707160	23792.934215	31.012800
526.130451	23819.448078	31.017818
526.686274	23855.370798	31.022836
527.230329	23890.685820	31.027853
527.499967	23902.924214	31.032871
527.997658	23956.863295	31.037888
528.553059	23978.684712	31.042906
529.105855	24008.145421	31.047924
529.535890	24055.193240	31.052941
529.917994	24087.583078	31.057959
530.593325	24099.813719	31.062976
531.204305	24167.752979	31.067994
531.653397	24172.414659	31.073012
531.976442	24227.913729	31.078029
532.622623	24259.739623	31.083047
533.184935	24295.709568	31.088064
533.562785	24332.102819	31.093082
533.947652	24398.436747	31.098100
534.494411	24412.492713	31.103117
534.899902	24464.793260	31.108135
535.630177	24499.543557	31.113152
536.297137	24540.485872	31.118170
536.163407	24593.476891	31.123188
537.172953	24604.658252	31.128205
537.490231	24691.046465	31.133223
538.193926	24693.557485	31.138240
538.897829	24736.328990	31.143258
539.238904	24760.851226	31.148276
540.068652	24810.897869	31.153293
540.236213	24856.125346	31.158311
540.676229	24861.064378	31.163328
541.336870	24925.146248	31.168346
541.451098	24954.058630	31.173364
542.469614	24982.447355	31.178381
542.492410	25026.950038	31.183399
543.609382	25034.040494	31.188416
543.873858	25121.774640	31.193434
544.418856	25137.336089	31.198452
545.614297	25198.917921	31.203469
545.713014	25213.224772	31.208487
546.302990	25276.221210	31.213504
546.599694	25311.447231	31.218522
547.365791	25322.763984	31.223540
548.201555	25389.596603	31.228557
548.491304	25441.515465	31.233575
549.340898	25438.224490	31.238592
549.880362	25508.927718	31.243610
550.210860	25537.227716	31.248628
550.677794	25557.992483	31.253645
550.986295	25619.623459	31.258663
551.652596	25676.444373	31.263680
552.544302	25684.383181	31.268698
552.843566	25748.951302	31.273716
553.505513	25765.662199	31.278733
554.188792	25844.734431	31.283751
554.713664	25866.265531	31.288768
555.545431	25885.130826	31.293786
555.359407	25955.853891	31.298804
556.708750	25962.700583	31.303821
556.854078	26046.572710	31.308839
557.405053	26035.949325	31.313856
558.067929	26123.835058	31.318874
558.709524	26124.698726	31.323892
559.097307	26189.201742	31.328909
559.382815	26232.831674	31.333927
559.773981	26252.863383	31.338944
560.717273	26317.987448	31.343962
560.913593	26343.052745	31.348980
562.028340	26411.552339	31.353997
562.396971	26452.214626	31.359015
563.044133	26459.432556	31.364032
563.783932	26543.946038	31.369050
564.488334	26534.537886	31.374068
565.366160	26609.140519	31.379085
565.432643	26626.814524	31.384103
566.177937	26685.809437	31.389120
566.968348	26693.667991	31.394138
567.381815	26774.632818	31.399156
567.744354	26786.429278	31.404173
568.693918	26781.886840	31.409191
569.044119	26848.044220	31.414208
569.389878	26868.057933	31.419226
569.853372	26915.047394	31.424244
570.273270	26949.393951	31.429261
570.814042	26980.138332	31.434279
571.533299	27022.065818	31.439296
572.466191	27050.204800	31.444314
572.409442	27076.286868	31.449332
573.261107	27126.666583	31.454349
573.622042	27164.285377	31.459367
574.212599	27209.393827	31.464384
574.791572	27235.163770	31.469402
575.273597	27295.921899	31.474420
576.027082	27293.406135	31.479437
575.993167	27368.514385	31.484455
576.605269	27424.038372	31.489472
577.455258	27431.499402	31.494490
577.576198	27519.168662	31.499508
578.545211	27543.068879	31.504525
578.955113	27609.822581	31.509543
579.511345	27666.394687	31.514560
580.379729	27707.505270	31.519578
580.831621	27743.852728	31.524596
581.870311	27803.651174	31.529613
582.280843	27833.803399	31.534631
582.857047	27897.032130	31.539648
583.529468	27907.952021	31.544666
583.840760	27959.340625	31.549684
584.575646	28014.598127	31.554701
585.345402	28044.086878	31.559719
586.029309	28101.576168	31.564736
586.388531	28144.308456	31.569754
587.103710	28185.172052	31.574772
587.579522	28211.143563	31.579789
587.817043	28287.000729	31.584807
588.694230	28302.562000	31.589824
589.185510	28376.440981	31.594842
589.693937	28408.353009	31.599860
590.620028	28491.279140	31.604877
590.899598	28509.586253	31.609895
591.987435	28529.485431	31.614912
592.667717	28614.663746	31.619930
593.072789	28633.464723	31.624948
593.715070	28672.913489	31.629965
594.447186	28716.468778	31.634983
595.199047	28773.161731	31.640000
595.774947	28802.507827	31.645018
595.817230	28845.806155	31.650036
597.008605	28894.621360	31.655053
597.554166	28926.898818	31.660071
597.826760	28960.718424	31.665088
598.468563	29004.619796	31.670106
598.664374	29073.600888	31.675124
599.854823	29089.420327	31.680141
600.167815	29122.310393	31.685159
600.612279	29188.474160	31.690176
601.712497	29205.732654	31.695194
601.873675	29247.245010	31.700212
602.513838	29297.353166	31.705229
602.894141	29305.759754	31.710247
603.638058	29365.957616	31.715264
604.217083	29405.388299	31.720282
604.879345	29436.792489	31.725300
605.426336	29471.875866	31.730317
605.683120	29538.288416	31.735335
606.203274	29574.677969	31.740352
607.082872	29596.620892	31.745370
607.840135	29669.848808	31.750388
608.191801	29720.439159	31.755405
608.992477	29732.821223	31.760423
609.543898	29790.742612	31.765440
609.883225	29836.664291	31.770458
610.470890	29877.809340	31.775476
611.471132	29924.893061	31.780493
611.630312	29997.748068	31.785511
612.435581	30009.355832	31.790528
613.061784	30084.388862	31.795546
613.486584	30136.136629	31.800564
614.113250	30177.263617	31.805581
615.015653	30256.998639	31.810599
615.594660	30274.394863	31.815616
616.207282	30349.119235	31.820634
616.713893	30376.570720	31.825652
617.541969	30434.863247	31.830669
617.986037	30495.576372	31.835687
618.569062	30545.041863	31.840704
619.492626	30581.694083	31.845722
619.587228	30626.933578	31.850740
620.508060	30704.642705	31.855757
621.353765	30739.953897	31.860775
622.023112	30791.516656	31.865792
622.985017	30837.776992	31.870810
623.360067	30884.992990	31.875828
623.999517	30936.351357	31.880845
624.973192	30974.645000	31.885863
624.993844	31019.985615	31.890880
625.768401	31069.642840	31.895898
626.316234	31115.894251	31.900916
627.107739	31158.338674	31.905933
627.693270	31206.535479	31.910951
628.317005	31244.830318	31.915968
628.721682	31316.077630	31.920986
629.600904	31354.823774	31.926004
630.162353	31413.688656	31.931021
630.825025	31431.148447	31.936039
631.175092	31512.563072	31.941056
632.139733	31524.028344	31.946074
632.938220	31585.478693	31.951092
633.606479	31627.713852	31.956109
634.379607	31647.629168	31.961127
634.635068	31733.373709	31.966144
635.739605	31731.002366	31.971162
635.403507	31817.356924	31.976180
636.436176	31816.844209	31.981197
637.239364	31890.900650	31.986215
637.413735	31912.503504	31.991232
638.331714	31961.519610	31.996250
638.743443	32020.905413	32.001268
639.555651	32053.018942	32.006285
640.038417	32087.215048	32.011303
640.352809	32152.595093	32.016320
641.415798	32199.713217	32.021338
641.677178	32244.525547	32.026356
642.340781	32286.504656	32.031373
643.231389	32347.517630	32.036391
643.445169	32421.392909	32.041408
644.469996	32448.855201	32.046426
644.818041	32518.633572	32.051444
645.536716	32559.636841	32.056461
646.094169	32619.747133	32.061479
646.654107	32662.563324	32.066496
647.581221	32727.373656	32.071514
648.288357	32756.352908	32.076532
649.071348	32786.070404	32.081549
649.960518	32885.020003	32.086567
650.321781	32927.412993	32.091584
651.517660	32946.814937	32.096602
651.741365	33029.056323	32.101620
652.573063	33058.840640	32.106637
653.183388	33136.103181	32.111655
653.641081	33146.844870	32.116672
654.611100	33216.867627	32.121690
654.981818	33294.178516	32.126708
655.179706	33325.719292	32.131725
656.026656	33376.729121	32.136743
657.178482	33416.196487	32.141760
657.777555	33500.700703	32.146778
658.094134	33555.457198	32.151796
658.887969	33592.220359	32.156813
659.636728	33676.365892	32.161831
659.674641	33720.186919	32.166848
661.190384	33742.395112	32.171866
661.549921	33809.607754	32.176884
662.072869	33874.118090	32.181901
663.090050	33920.780277	32.186919
663.369035	33990.679895	32.191936
664.213653	34008.387745	32.196954
664.699072	34099.013447	32.201972
665.250669	34141.059250	32.206989
665.883290	34205.561295	32.212007
667.026352	34236.294408	32.217024
667.623072	34320.748009	32.222042
667.966587	34369.192800	32.227060
668.680181	34403.330157	32.232077
669.731040	34493.809661	32.237095
670.218421	34515.041353	32.242112
671.106572	34578.853127	32.247130
671.083505	34630.158251	32.252148
672.297832	34660.057941	32.257165
672.438346	34728.114702	32.262183
672.915701	34746.093056	32.267200
673.803292	34829.244976	32.272218
674.323012	34860.576638	32.277236
674.662368	34951.044227	32.282253
675.982535	34974.475416	32.287271
676.323352	35070.120336	32.292288
677.098105	35094.127222	32.297306
677.757592	35180.785334	32.302324
678.560954	35202.073218	32.307341
678.926753	35290.649880	32.312359
679.779411	35311.104002	32.317376
680.440821	35397.334143	32.322394
681.384936	35439.235610	32.327412
682.067236	35525.828826	32.332429
682.700371	35558.917262	32.337447
683.083134	35595.963140	32.342464
683.882904	35702.748859	32.347482
684.349957	35747.479581	32.352500
686.081336	35767.125938	32.357517
686.576989	35864.541641	32.362535
686.609743	35938.354187	32.367552
687.229221	35973.707895	32.372570
687.789214	36040.112529	32.377588
688.518183	36107.748582	32.382605
690.004008	36141.347213	32.387623
690.405309	36250.042815	32.392640
691.021663	36307.390280	32.397658
691.565739	36351.166012	32.402676
691.917917	36408.748221	32.407693
692.837198	36461.329399	32.412711
694.028444	36512.978269	32.417728
695.017941	36592.135653	32.422746
695.882648	36638.813986	32.427764
695.896511	36708.023059	32.432781
697.046073	36744.094902	32.437799
697.575193	36832.727823	32.442816
698.523205	36850.458520	32.447834
698.997730	36945.503231	32.452852
699.640843	36970.988980	32.457869
700.436910	37052.780715	32.462887
701.085320	37093.642408	32.467904
701.575975	37139.643837	32.472922
702.783567	37181.424174	32.477940
703.029929	37287.363706	32.482957
703.521077	37328.938417	32.487975
704.286575	37367.221693	32.492992
705.153912	37470.332791	32.498010
706.023320	37489.066814	32.503028
706.369766	37587.408652	32.508045
707.404134	37599.962868	32.513063
708.113942	37695.578217	32.518080
709.155921	37739.710313	32.523098
709.553616	37762.877645	32.528116
710.169712	37824.457384	32.533133
711.008136	37845.870779	32.538151
711.469204	37925.683028	32.543168
711.863512	37961.379502	32.548186
712.838447	38018.500715	32.553204
713.310990	38083.399539	32.558221
714.359053	38129.458415	32.563239
714.716980	38200.594450	32.568256
715.762762	38236.585124	32.573274
715.995084	38312.139076	32.578292
716.574122	38344.970436	32.583309
717.743493	38419.027593	32.588327
718.241111	38489.053085	32.593344
719.090941	38535.125708	32.598362
719.721970	38625.863094	32.603380
720.432538	38657.649237	32.608397
721.200047	38726.286200	32.613415
721.592135	38792.480883	32.618432
722.567773	38868.354172	32.623450
723.497927	38907.270677	32.628468
724.075388	38972.091563	32.633485
724.704141	39046.619116	32.638503
725.723693	39084.310826	32.643520
726.375902	39187.335784	32.648538
727.099599	39232.531614	32.653556
727.397887	39288.205383	32.658573
728.484612	39363.284262	32.663591
728.880537	39444.634097	32.668608
730.239677	39472.668179	32.673626
731.100305	39582.538902	32.678644
731.641404	39613.858696	32.683661
732.705927	39689.388801	32.688679
733.199768	39723.370154	32.693696
733.892891	39787.861952	32.698714
734.682325	39871.429745	32.703732
735.122949	39929.415138	32.708749
736.389609	39967.151476	32.713767
736.871285	40057.757878	32.718784
738.027182	40099.575768	32.723802
738.512720	40173.259048	32.728820
738.902381	40214.899588	32.733837
739.954173	40279.031813	32.738855
740.619534	40336.391479	32.743872
741.125401	40411.305694	32.748890
741.990338	40465.511735	32.753908
742.283179	40547.968173	32.758925
743.114633	40583.961700	32.763943
744.036395	40666.610327	32.768960
744.474882	40751.282235	32.773978
745.570804	40780.640873	32.778996
746.193271	40875.947438	32.784013
747.288700	40915.925618	32.789031
747.764232	41004.828602	32.794048
748.714205	41032.473089	32.799066
748.599080	41116.134205	32.804084
749.593286	41145.730443	32.809101
750.726688	41232.892984	32.814119
751.339730	41277.253983	32.819136
751.753505	41368.625644	32.824154
753.220108	41391.839106	32.829172
753.365448	41487.243952	32.834189
754.132557	41501.387544	32.839207
754.839675	41612.590511	32.844224
755.806056	41648.705165	32.849242
756.687972	41725.372552	32.854260
756.999598	41805.288299	32.859277
758.259730	41849.557240	32.864295
758.616992	41912.058793	32.869312
759.362088	41999.012640	32.874330
760.456082	42054.887337	32.879348
760.887687	42114.368752	32.884365
761.875418	42210.573996	32.889383
762.766897	42259.271191	32.894400
763.485736	42331.857367	32.899418
764.596935	42410.983124	32.904436
765.090631	42472.474580	32.909453
765.899638	42519.308889	32.914471
766.597884	42603.418687	32.919488
767.751159	42660.711636	32.924506
768.758793	42700.982392	32.929524
769.351152	42786.671294	32.934541
770.144512	42830.159113	32.939559
770.625925	42905.368851	32.944576
771.323035	42966.608894	32.949594
772.088712	43031.121876	32.954612
772.623559	43109.137641	32.959629
773.325647	43180.096121	32.964647
774.194817	43252.867284	32.969664
774.849940	43317.402088	32.974682
776.065248	43385.516503	32.979700
776.773070	43463.831239	32.984717
777.447841	43536.801725	32.989735
778.605645	43584.920882	32.994752
779.250442	43686.078289	32.999770
780.047450	43732.756934	33.004788
780.439303	43800.843183	33.009805
781.484251	43879.579309	33.014823
782.162919	43931.904892	33.019840
782.866278	44028.121382	33.024858
783.803657	44062.933469	33.029876
784.277447	44173.183812	33.034893
785.049110	44211.505162	33.039911
785.962684	44318.131278	33.044928
786.758398	44364.373353	33.049946
787.536494	44458.258584	33.054964
788.145334	44510.499239	33.059981
789.026627	44593.394002	33.064999
789.756264	44632.612569	33.070016
790.438384	44710.574254	33.075034
791.679810	44768.913818	33.080052
792.373796	44836.303035	33.085069
793.003563	44901.220025	33.090087
793.515997	44954.209238	33.095104
794.061152	45048.784596	33.100122
795.297220	45107.905359	33.105140
795.654055	45186.012435	33.110157
797.084047	45221.120703	33.115175
797.817532	45329.728145	33.120192
798.144247	45372.176706	33.125210
799.237149	45430.226661	33.130228
799.888455	45545.101229	33.135245
801.067835	45576.861889	33.140263
801.883988	45646.490461	33.145280
802.038720	45730.247657	33.150298
803.547436	45790.327418	33.155316
803.983684	45878.741187	33.160333
805.074051	45920.996979	33.165351
806.152861	46011.577474	33.170368
806.175526	46084.776027	33.175386
807.534020	46142.155111	33.180404
808.318280	46217.050209	33.185421
809.041975	46296.245932	33.190439
809.819648	46379.903936	33.195456
810.936140	46415.919504	33.200474
811.632275	46524.575024	33.205492
812.382877	46579.048793	33.210509
812.945695	46676.567414	33.215527
813.982954	46713.164101	33.220544
814.528548	46819.542277	33.225562
815.310170	46875.094193	33.230580
816.589910	46944.755113	33.235597
817.320418	47024.792279	33.240615
818.161285	47106.424475	33.245632
818.934030	47156.981105	33.250650
820.140304	47248.065142	33.255668
820.684168	47317.680600	33.260685
821.492673	47368.292095	33.265703
822.623459	47430.860766	33.270720
823.224204	47554.777004	33.275738
824.172987	47604.805242	33.280756
824.593304	47658.331597	33.285773
825.842261	47718.099647	33.290791
826.274601	47800.241805	33.295808
826.807797	47915.636597	33.300826
827.927280	47964.600634	33.305844
828.661192	48040.817781	33.310861
829.348009	48121.857629	33.315879
830.587053	48191.788704	33.320896
831.343609	48249.740629	33.325914
832.755547	48346.085822	33.330932
833.712715	48384.752830	33.335949
834.555996	48491.242025	33.340967
835.057448	48529.101549	33.345984
835.783770	48577.451476	33.351002
836.659155	48657.501404	33.356020
837.394326	48688.761004	33.361037
838.188359	48770.092831	33.366055
838.968443	48822.041429	33.371072
839.717617	48887.560006	33.376090
840.276030	48936.499292	33.381108
841.175975	49043.468722	33.386125
842.171925	49082.623331	33.391143
842.853386	49170.664362	33.396160
843.674849	49231.439585	33.401178
844.318395	49298.068268	33.406196
845.382957	49382.420629	33.411213
845.987075	49445.951178	33.416231
846.755539	49530.370298	33.421248
847.149271	49610.744159	33.426266
848.368524	49681.353247	33.431284
849.197279	49759.481252	33.436301
849.763978	49863.716026	33.441319
850.827768	49920.965023	33.446336
851.387383	50034.712748	33.451354
852.622975	50074.468841	33.456372
853.569628	50198.313816	33.461389
854.179235	50247.428439	33.466407
855.322731	50360.211221	33.471424
855.800700	50443.639549	33.476442
857.074190	50493.826256	33.481460
858.074384	50599.460568	33.486477
859.089730	50658.732968	33.491495
860.085297	50773.867643	33.496512
860.681491	50813.774481	33.501530
861.868008	50918.162928	33.506548
862.320207	51003.702840	33.511565
863.463175	51057.007688	33.516583
864.257860	51167.193940	33.521600
865.163691	51228.543222	33.526618
866.388735	51295.579143	33.531636
866.903895	51402.844885	33.536653
867.833615	51463.774606	33.541671
868.576364	51555.320625	33.546688
869.339924	51611.644525	33.551706
870.496256	51724.919880	33.556724
871.312232	51778.266294	33.561741
872.223767	51866.183032	33.566759
873.064587	51956.478383	33.571776
874.117574	52013.757913	33.576794
875.089039	52089.793656	33.581812
875.833092	52208.401762	33.586829
876.555325	52262.080128	33.591847
877.686965	52346.921850	33.596864
878.564699	52410.930672	33.601882
879.348266	52482.645875	33.606900
880.274097	52575.496636	33.611917
881.265659	52637.181105	33.616935
882.034660	52689.079618	33.621952
883.010262	52760.790619	33.626970
883.818292	52846.027046	33.631988
884.768891	52890.306914	33.637005
885.190730	52968.359037	33.642023
886.197338	53045.523109	33.647040
886.787244	53100.695776	33.652058
888.129974	53189.453015	33.657076
888.740024	53259.115880	33.662093
889.500138	53323.317095	33.667111
890.347748	53389.332030	33.672128
891.073279	53488.070881	33.677146
891.939135	53565.291134	33.682164
892.872562	53637.533105	33.687181
893.575155	53721.736272	33.692199
894.759465	53816.395519	33.697216
895.419857	53903.532073	33.702234
896.633461	53969.860171	33.707252
897.143432	54036.499322	33.712269
897.827530	54158.626925	33.717287
898.985757	54226.293574	33.722304
899.765876	54309.597059	33.727322
900.732895	54425.349867	33.732340
902.328361	54487.102381	33.737357
903.022186	54576.045433	33.742375
904.104891	54647.863666	33.747392
904.623937	54755.050857	33.752410
906.112469	54798.271329	33.757428
907.183985	54916.674643	33.762445
908.009917	54986.129878	33.767463
909.070636	55049.405576	33.772480
909.856410	55142.118187	33.777498
911.133796	55209.428646	33.782516
912.037874	55281.972232	33.787533
912.435970	55365.941076	33.792551
913.506942	55427.919138	33.797568
914.216573	55523.221515	33.802586
915.161261	55595.305347	33.807604
916.179383	55678.207913	33.812621
916.797614	55765.903024	33.817639
917.573009	55843.592432	33.822656
918.254523	55933.443692	33.827674
918.912586	56023.075006	33.832692
920.445866	56115.894586	33.837709
921.233762	56196.257169	33.842727
922.036833	56286.930490	33.847744
923.090203	56373.855343	33.852762
924.137794	56460.917266	33.857780
925.213110	56552.227271	33.862797
925.924318	56640.315833	33.867815
927.034494	56721.993146	33.872832
927.996814	56807.589775	33.877850
929.179019	56895.462569	33.882868
930.158209	56979.570480	33.887885
930.725467	57056.436347	33.892903
931.937151	57124.963902	33.897920
932.656575	57205.597502	33.902938
933.147302	57267.099580	33.907956
934.682904	57341.252381	33.912973
935.041260	57427.591989	33.917991
935.871621	57501.721901	33.923008
936.600606	57585.787160	33.928026
937.164475	57673.383227	33.933044
938.223748	57748.478447	33.938061
938.867197	57864.736989	33.943079
940.219160	57940.982901	33.948096
940.767638	58038.360201	33.953114
942.097394	58145.201446	33.958132
943.235933	58217.425743	33.963149
944.102058	58318.851754	33.968167
945.318198	58401.795095	33.973184
946.346968	58488.680186	33.978202
947.411943	58567.588374	33.983220
948.487932	58661.892147	33.988237
949.062751	58741.617815	33.993255
950.475869	58815.410876	33.998272
951.637454	58906.485200	34.003290
952.235322	58996.948779	34.008308
953.444873	59073.960795	34.013325
954.162681	59176.355924	34.018343
954.732145	59256.836061	34.023360
956.023853	59333.365665	34.028378
957.002424	59426.757459	34.033396
958.088781	59514.730588	34.038413
958.697476	59607.957977	34.043431
960.050042	59692.868131	34.048448
960.984493	59787.165411	34.053466
961.771108	59883.441040	34.058484
962.845285	59960.945548	34.063501
963.751819	60043.917077	34.068519
964.667206	60133.221138	34.073536
965.768514	60249.219701	34.078554
966.647969	60322.061737	34.083572
967.505985	60411.360470	34.088589
968.756984	60505.980436	34.093607
969.791085	60596.189779	34.098624
970.753431	60698.914313	34.103642
971.454160	60774.303002	34.108660
972.566738	60859.133512	34.113677
973.356374	60952.796658	34.118695
974.613642	61049.729636	34.123712
975.753912	61145.074569	34.128730
976.608062	61219.357625	34.133748
977.784201	61323.298783	34.138765
978.376004	61417.601968	34.143783
979.697052	61484.593684	34.148800
980.835446	61563.114510	34.153818
981.165671	61691.069726	34.158836
982.568715	61754.771799	34.163853
983.097837	61863.274235	34.168871
984.437272	61929.007888	34.173888
985.209398	62011.074864	34.178906
986.141013	62106.881000	34.183924
987.413089	62155.666454	34.188941
987.816576	62257.162209	34.193959
988.913190	62342.965059	34.198976
989.822016	62425.226816	34.203994
990.631363	62514.489619	34.209012
991.832036	62590.718646	34.214029
992.187407	62707.154212	34.219047
993.455489	62794.163359	34.224064
994.233043	62873.647020	34.229082
995.228414	62989.553055	34.234100
996.450962	63080.208542	34.239117
996.907994	63174.655635	34.244135
998.498615	63258.558839	34.249152
999.494640	63385.866996	34.254170
1000.502651	63465.414376	34.259188
1001.686416	63571.725654	34.264205
1002.597140	63674.083052	34.269223
1003.654137	63766.438696	34.274240
1004.363832	63877.889254	34.279258
1005.757091	63975.936721	34.284276
1006.959990	64058.269326	34.289293
1007.667271	64175.876902	34.294311
1008.733796	64275.455831	34.299328
1009.864694	64351.551466	34.304346
1010.694416	64483.570462	34.309364
1012.207323	64562.091551	34.314381
1013.175926	64654.617158	34.319399
1014.066491	64769.758056	34.324416
1015.066575	64872.603508	34.329434
1016.004862	64943.843403	34.334452
1017.064421	65068.278827	34.339469
1017.883806	65145.080920	34.344487
1018.660410	65276.839092	34.349504
1019.939975	65343.778451	34.354522
1020.651919	65467.396950	34.359540
1021.856988	65590.473546	34.364557
1023.312973	65667.827069	34.369575
1023.546984	65786.274660	34.374592
1025.577829	65868.252829	34.379610
1025.940311	66009.875711	34.384628
1027.394750	66087.793354	34.389645
1028.233704	66191.821149	34.394663
1029.203604	66310.344413	34.399680
1030.776520	66393.932631	34.404698
1031.550806	66499.712633	34.409716
1032.740436	66596.362570	34.414733
1033.739142	66713.257165	34.419751
1034.823787	66794.369641	34.424768
1035.909920	66894.840280	34.429786
1036.791320	67001.294538	34.434804
1037.741068	67089.978426	34.439821
1038.654930	67178.741076	34.444839
1039.288221	67285.940711	34.449856
1040.788522	67388.410544	34.454874
1041.382865	67465.156638	34.459892
1042.494531	67574.549607	34.464909
1043.760792	67664.487112	34.469927
1044.492085	67750.372391	34.474944
1045.635346	67856.988701	34.479962
1046.355018	67959.882641	34.484980
1047.523955	68052.926555	34.489997
1048.561781	68148.998797	34.495015
1049.694684	68255.322035	34.500032
1050.867372	68356.307682	34.505050
1051.528463	68464.690761	34.510068
1052.783069	68571.811318	34.515085
1053.801891	68673.909686	34.520103
1054.823987	68769.210453	34.525120
1056.158893	68889.264522	34.530138
1056.883550	68990.874353	34.535156
1058.351497	69091.463074	34.540173
1059.417407	69201.908579	34.545191
1060.419866	69318.391853	34.550208
1061.801353	69411.168394	34.555226
1062.307265	69513.428556	34.560244
1063.559672	69638.244974	34.565261
1065.073050	69723.818725	34.570279
1065.706881	69832.270602	34.575296
1066.944171	69943.628084	34.580314
1067.868066	70053.323895	34.585332
1069.081619	70151.298707	34.590349
1070.211663	70257.304790	34.595367
1071.003411	70374.674477	34.600384
1072.214564	70486.209788	34.605402
1073.584923	70591.724559	34.610420
1074.828558	70691.738027	34.615437
1075.685452	70795.016812	34.620455
1076.582836	70919.057544	34.625472
1078.006337	70985.488080	34.630490
1078.832197	71122.860244	34.635508
1080.717732	71212.153304	34.640525
1081.733425	71302.065307	34.645543
1082.460355	71427.014594	34.650560
1084.036121	71480.141438	34.655578
1084.391453	71623.651234	34.660596
1086.127486	71720.432418	34.665613
1086.876051	71813.877017	34.670631
1087.915368	71932.278118	34.675648
1089.368869	72027.532439	34.680666
1089.975739	72114.682463	34.685684
1091.371493	72254.252862	34.690701
1092.345150	72326.496767	34.695719
1093.058234	72442.273706	34.700736
1094.553637	72559.948885	34.705754
1095.591110	72654.078154	34.710772
1096.627266	72737.251347	34.715789
1097.796889	72850.973973	34.720807
1098.586308	72926.465634	34.725824
1100.162855	73028.725415	34.730842
1100.628718	73134.505055	34.735860
1101.743140	73222.640799	34.740877
1103.091389	73308.439653	34.745895
1103.826675	73415.991476	34.750912
1104.817180	73511.016932	34.755930
1105.839220	73627.427772	34.760948
1106.918524	73723.154170	34.765965
1108.004718	73828.832521	34.770983
1108.696579	73950.359359	34.776000
1110.071568	74059.974066	34.781018
1110.979056	74179.597529	34.786036
1112.111969	74280.613579	34.791053
1113.375610	74377.457583	34.796071
1114.243427	74513.386776	34.801088
1115.410622	74623.018659	34.806106
1116.532582	74738.838701	34.811124
1117.556985	74863.553726	34.816141
1118.942148	74981.987477	34.821159
1119.977887	75106.847558	34.826176
1121.510802	75213.877750	34.831194
1122.552026	75335.401663	34.836212
1123.506199	75447.422811	34.841229
1124.752442	75557.837181	34.846247
1125.562557	75696.102864	34.851264
1126.881006	75808.921251	34.856282
1128.358225	75902.281760	34.861300
1129.125931	76049.878256	34.866317
1130.520469	76156.158131	34.871335
1131.680477	76270.742254	34.876352
1132.930817	76389.281565	34.881370
1134.233824	76510.176856	34.886388
1135.112495	76621.249576	34.891405
1136.719626	76737.781318	34.896423
1137.504685	76861.023637	34.901440
1138.885970	76974.559030	34.906458
1140.097188	77086.403029	34.911476
1141.248239	77194.932808	34.916493
1142.355854	77301.972190	34.921511
1143.565146	77426.667328	34.926528
1144.889997	77531.315927	34.931546
1145.925133	77653.107546	34.936564
1146.961978	77770.469063	34.941581
1148.406837	77881.104702	34.946599
1149.325863	77990.484633	34.951616
1150.951144	78079.179820	34.956634
1151.562234	78217.241520	34.961652
1153.082498	78324.271225	34.966669
1154.290876	78423.336639	34.971687
1155.029347	78546.312144	34.976704
1156.473966	78654.366900	34.981722
1157.358670	78775.076710	34.986740
1158.595548	78895.263499	34.991757
1159.804702	78985.823875	34.996775
1160.771633	79092.553707	35.001792
1161.933852	79191.870372	35.006810
1163.248403	79293.893886	35.011828
1164.068277	79395.541466	35.016845
1165.219270	79498.325221	35.021863
1165.989500	79606.643939	35.026880
1167.401738	79713.919321	35.031898
1168.308695	79839.334629	35.036916
1169.230407	79945.494554	35.041933
1170.881924	80046.722347	35.046951
1171.804020	80164.684725	35.051968
1172.993535	80285.196911	35.056986
1174.352102	80391.131640	35.062004
1175.407590	80520.155810	35.067021
1176.890664	80637.026619	35.072039
1177.807545	80759.253726	35.077056
1179.046108	80859.906408	35.082074
1180.060825	80995.166493	35.087092
1180.973067	81115.809788	35.092109
1182.561737	81226.004419	35.097127
1183.531913	81358.366113	35.102144
1185.107889	81473.633874	35.107162
1186.426419	81578.651796	35.112180
1187.485503	81706.096082	35.117197
1188.847972	81816.247637	35.122215
1190.032092	81943.951649	35.127232
1191.439717	82071.608265	35.132250
1192.392869	82172.413844	35.137268
1193.434948	82291.102560	35.142285
1195.150375	82406.580907	35.147303
1196.128181	82536.805808	35.152320
1197.460838	82649.021094	35.157338
1198.511800	82766.674322	35.162356
1199.405636	82887.615297	35.167373
1200.643571	83015.500648	35.172391
1201.842967	83136.299648	35.177408
1203.161941	83260.690203	35.182426
1204.442836	83382.862189	35.187444
1205.513115	83515.828571	35.192461
1207.433620	83621.146715	35.197479
1208.343277	83754.057957	35.202496
1209.226464	83873.944190	35.207514
1210.864468	83997.687782	35.212532
1212.238781	84104.498730	35.217549
1213.697968	84229.808431	35.222567
1214.226041	84353.275379	35.227584
1215.686129	84455.010272	35.232602
1216.840000	84575.799498	35.237620
1218.026983	84694.636837	35.242637
1219.256974	84811.362622	35.247655
1220.342262	84950.835189	35.252672
1221.554338	85058.897014	35.257690
1223.054924	85191.483105	35.262708
1223.908087	85309.441230	35.267725
1225.152414	85418.132025	35.272743
1226.423305	85532.326220	35.277760
1227.681118	85643.488201	35.282778
1228.899434	85753.329264	35.287796
1229.616557	85867.341424	35.292813
1231.189320	85973.535928	35.297831
1232.371165	86096.662504	35.302848
1233.265174	86214.018487	35.307866
1234.676561	86334.258317	35.312884
1235.925781	86453.007096	35.317901
1236.848624	86571.833717	35.322919
1237.934394	86699.076355	35.327936
1239.439618	86823.085204	35.332954
1240.697720	86943.283285	35.337972
1241.509913	87076.534361	35.342989
1242.616905	87200.735175	35.348007
1244.197319	87335.762690	35.353024
1245.451011	87467.662394	35.358042
1247.069485	87588.963970	35.363060
1247.703930	87723.334932	35.368077
1249.342070	87833.429803	35.373095
1250.368049	87990.238770	35.378112
1251.628469	88119.460280	35.383130
1253.591434	88250.531164	35.388148
1254.251491	88385.711598	35.393165
1255.930108	88521.768021	35.398183
1257.286304	88647.518479	35.403200
1258.071365	88784.344649	35.408218
1259.636219	88915.432280	35.413236
1260.834064	89047.502316	35.418253
1262.341622	89180.763381	35.423271
1263.679711	89317.365885	35.428288
1265.156939	89436.670383	35.433306
1266.466108	89560.264550	35.438324
1267.316415	89713.313300	35.443341
1268.834803	89833.378634	35.448359
1270.077395	89950.952554	35.453376
1271.364803	90092.759999	35.458394
1272.755218	90226.893538	35.463412
1274.132071	90351.923341	35.468429
1275.365909	90476.660389	35.473447
1276.575038	90626.490124	35.478464
1277.729729	90741.970012	35.483482
1279.314058	90866.805358	35.488500
1280.289416	91009.205933	35.493517
1281.728918	91143.312011	35.498535
1283.032997	91264.994068	35.503552
1284.655873	91419.943136	35.508570
1285.895765	91521.449288	35.513588
1286.955463	91659.185890	35.518605
1288.495050	91776.558001	35.523623
1289.610469	91921.415128	35.528640
1290.819247	92047.879076	35.533658
1292.442068	92148.037041	35.538676
1293.230901	92311.043416	35.543693
1294.633531	92428.282663	35.548711
1296.046463	92540.448455	35.553728
1297.278449	92668.329022	35.558746
1298.437780	92758.526024	35.563764
1299.537190	92903.044288	35.568781
1300.813638	93019.882975	35.573799
1301.912125	93149.754589	35.578816
1302.916288	93256.214350	35.583834
1304.621392	93379.115672	35.588852
1305.905697	93524.943181	35.593869
1307.233145	93633.870729	35.598887
1308.250638	93764.106698	35.603904
1309.620827	93890.561869	35.608922
1310.541507	94035.172854	35.613940
1311.861848	94175.970405	35.618957
1313.517108	94304.697647	35.623975
1314.900173	94437.706837	35.628992
1315.875948	94570.642403	35.634010
1317.022090	94728.707636	35.639028
1318.518172	94866.179776	35.644045
1319.719925	95000.631708	35.649063
1321.250767	95155.374886	35.654080
1322.717597	95293.335041	35.659098
1323.961068	95430.819179	35.664116
1325.238598	95576.091887	35.669133
1326.854737	95714.884863	35.674151
1328.320226	95859.927115	35.679168
1329.425157	95995.260698	35.684186
1331.268077	96133.185222	35.689204
1332.837242	96272.140929	35.694221
1334.267027	96402.731590	35.699239
1335.553083	96529.683174	35.704256
1336.854985	96664.812353	35.709274
1338.275549	96803.877196	35.714292
1339.720804	96950.093664	35.719309
1340.739115	97065.900151	35.724327
1342.233627	97217.323159	35.729344
1343.405149	97349.687363	35.734362
1345.245509	97473.247602	35.739380
1346.372292	97608.492494	35.744397
1348.075301	97752.174339	35.749415
1349.223321	97889.302740	35.754432
1350.570494	98013.589588	35.759450
1352.217137	98141.928975	35.764468
1353.178609	98285.244922	35.769485
1354.438509	98410.680229	35.774503
1356.027272	98547.609695	35.779520
1357.175363	98703.304746	35.784538
1358.530970	98831.029992	35.789556
1359.663337	98970.375340	35.794573
1361.046031	99111.541768	35.799591
1362.355343	99251.322547	35.804608
1363.704603	99391.844376	35.809626
1365.449037	99540.560612	35.814644
1366.757515	99682.912798	35.819661
1367.687424	99791.945944	35.824679
1369.370131	99951.366906	35.829696
1370.317717	100062.106765	35.834714
1371.895495	100177.631355	35.839732
1373.275971	100308.138381	35.844749
1374.402513	100431.151104	35.849767
1375.575798	100589.157957	35.854784
1376.404698	100715.218492	35.859802
1378.070747	100835.711726	35.864820
1379.175688	100993.377889	35.869837
1380.295101	101152.643594	35.874855
1381.964078	101263.831363	35.879872
1382.975760	101443.432764	35.884890
1385.029875	101575.048391	35.889908
1386.373415	101729.568631	35.894925
1387.499854	101888.192884	35.899943
1389.039752	102008.845145	35.904960
1390.328742	102189.154869	35.909978
1392.184268	102320.489910	35.914996
1393.368082	102471.471769	35.920013
1394.695141	102615.832211	35.925031
1396.308783	102764.121725	35.930048
1397.725234	102915.417502	35.935066
1399.253595	103062.406315	35.940084
1400.652475	103215.003992	35.945101
1402.238012	103371.958130	35.950119
1403.981486	103505.627273	35.955136
1405.313583	103655.523811	35.960154
1407.021341	103799.432399	35.965172
1408.255556	103948.536393	35.970189
1409.768569	104091.129870	35.975207
1411.360385	104223.276852	35.980224
1412.338130	104383.510973	35.985242
1413.728337	104517.912779	35.990260
1415.355126	104660.896618	35.995277
1417.057569	104824.207928	36.000295
1418.448115	104956.321389	36.005312
1419.917068	105102.111047	36.010330
1421.299160	105225.418483	36.015348
1422.806804	105386.910454	36.020365
1424.228443	105540.715612	36.025383
1426.241830	105668.835823	36.030400
1427.338479	105813.125904	36.035418
1428.489573	105937.454647	36.040436
1429.768298	106087.539619	36.045453
1431.010322	106237.542768	36.050471
1432.658953	106370.679947	36.055488
1433.711994	106530.372332	36.060506
1435.464405	106672.215502	36.065524
1436.946188	106834.778277	36.070541
1437.957747	106971.956469	36.075559
1439.955807	107129.825584	36.080576
1440.790998	107257.559299	36.085594
1442.899511	107431.380373	36.090612
1444.388493	107571.410050	36.095629
1445.414402	107707.988925	36.100647
1446.927208	107846.016482	36.105664
1447.966052	107977.886103	36.110682
1449.524792	108106.414398	36.115700
1450.739588	108245.358669	36.120717
1451.980207	108390.388209	36.125735
1453.456432	108533.817892	36.130752
1454.744495	108670.771952	36.135770
1456.137409	108829.659763	36.140788
1457.611531	108979.446932	36.145805
1459.027879	109117.737592	36.150823
1460.371239	109279.345149	36.155840
1461.764814	109432.996136	36.160858
1463.236744	109573.824960	36.165876
1464.354452	109761.016992	36.170893
1465.945971	109913.253411	36.175911
1467.846396	110050.706594	36.180928
1469.208935	110234.793546	36.185946
1471.087227	110371.802655	36.190964
1472.377416	110555.352840	36.195981
1473.812859	110689.737665	36.200999
1475.378693	110852.592556	36.206016
1476.902370	111036.628282	36.211034
1478.540729	111170.154300	36.216052
1480.088615	111334.907851	36.221069
1481.511906	111489.079747	36.226087
1483.117655	111668.391398	36.231104
1484.408816	111814.749874	36.236122
1486.453032	111980.606259	36.241140
1488.046994	112138.242930	36.246157
1489.196542	112292.412695	36.251175
1490.755096	112437.491679	36.256192
1492.338574	112608.002153	36.261210
1493.863415	112759.013413	36.266228
1495.419538	112912.818590	36.271245
1496.477266	113080.497594	36.276263
1498.374881	113256.356015	36.281280
1499.883085	113396.150112	36.286298
1501.301463	113565.547585	36.291316
1502.885152	113739.661455	36.296333
1504.336297	113873.092523	36.301351
1505.971841	114052.309037	36.306368
1507.540357	114208.627129	36.311386
1508.988784	114361.122594	36.316404
1510.722253	114532.040214	36.321421
1511.949530	114701.931544	36.326439
1513.957701	114848.143290	36.331456
1515.166074	114999.034774	36.336474
1516.749454	115172.031760	36.341492
1518.196506	115319.962411	36.346509
1519.662171	115473.164604	36.351527
1521.463392	115640.761602	36.356544
1522.818145	115804.739682	36.361562
1524.101320	115952.066971	36.366580
1525.784109	116128.859652	36.371597
1527.285380	116270.373892	36.376615
1528.923936	116407.087113	36.381632
1529.812647	116589.719826	36.386650
1531.671505	116703.043972	36.391668
1532.956501	116879.347924	36.396685
1534.426945	117010.709542	36.401703
1535.738892	117152.417047	36.406720
1537.227006	117323.962318	36.411738
1538.676459	117473.576613	36.416756
1540.442686	117633.284406	36.421773
1541.788260	117807.153867	36.426791
1543.087732	117953.014902	36.431808
1545.330172	118098.163463	36.436826
1546.420966	118303.151982	36.441844
1548.112491	118437.436325	36.446861
1549.202261	118627.288675	36.451879
1551.058165	118757.914200	36.456896
1552.153177	118981.377025	36.461914
1553.714989	119123.346976	36.466932
1555.542251	119295.611344	36.471949
1556.691633	119481.370131	36.476967
1558.596138	119663.065508	36.481984
1560.362793	119817.600929	36.487002
1562.023822	120025.019967	36.492020
1563.823773	120175.651709	36.497037
1565.096422	120343.920631	36.502055
1566.798353	120532.841189	36.507072
1568.550379	120697.946167	36.512090
1570.041665	120888.219848	36.517108
1571.787896	121040.486169	36.522125
1573.140841	121229.125251	36.527143
1574.967869	121414.574870	36.532160
1576.534515	121573.205161	36.537178
1578.085787	121766.312596	36.542196
1579.926221	121921.646631	36.547213
1581.460950	122094.647184	36.552231
1583.350510	122268.580390	36.557248
1584.906353	122439.401452	36.562266
1586.532852	122625.284072	36.567284
1588.512084	122768.201744	36.572301
1589.844931	122965.266236	36.577319
1591.718189	123116.371830	36.582336
1593.373612	123274.060994	36.587354
1594.931683	123452.234275	36.592372
1596.467102	123598.443997	36.597389
1598.083722	123775.356233	36.602407
1599.926716	123929.739043	36.607424
1601.342690	124118.186060	36.612442
1603.190688	124256.382839	36.617460
1604.956406	124458.544707	36.622477
1606.289052	124589.250705	36.627495
1608.098320	124775.081306	36.632512
1609.794860	124914.192179	36.637530
1610.929302	125091.772355	36.642548
1612.697238	125229.378881	36.647565
1613.824760	125405.087579	36.652583
1615.680265	125557.603125	36.657600
1616.967413	125700.393086	36.662618
1618.281267	125875.264579	36.667636
1620.036826	125987.150655	36.672653
1621.237192	126188.971970	36.677671
1623.132588	126318.406286	36.682688
1624.209902	126512.687342	36.687706
1625.439519	126654.136088	36.692724
1627.174297	126849.113160	36.697741
1629.027248	126991.541380	36.702759
1630.320345	127203.020670	36.707776
1632.086220	127360.285545	36.712794
1633.415260	127539.674965	36.717812
1634.997923	127722.280871	36.722829
1636.629966	127919.372069	36.727847
1638.591045	128095.953851	36.732864
1640.229327	128308.463622	36.737882
1641.726054	128468.273189	36.742900
1643.105011	128663.332362	36.747917
1644.951058	128872.380433	36.752935
1646.448441	129053.602555	36.757952
1648.676656	129218.139582	36.762970
1650.473918	129422.486934	36.767988
1652.560182	129647.819689	36.773005
1653.807575	129818.571620	36.778023
1655.373844	129981.774084	36.783040
1657.495143	130164.069903	36.788058
1659.003986	130398.850012	36.793076
1660.904209	130572.682786	36.798093
1662.580046	130728.131480	36.803111
1664.225819	130924.823812	36.808128
1665.944119	131133.199703	36.813146
1667.150795	131284.621164	36.818164
1669.624999	131498.061466	36.823181
1671.315448	131669.995948	36.828199
1672.527916	131864.812578	36.833216
1674.480587	132023.987349	36.838234
1676.189695	132256.432652	36.843252
1678.018991	132404.796546	36.848269
1679.418433	132629.603524	36.853287
1681.298410	132778.772205	36.858304
1683.046139	132990.058563	36.863322
1684.827615	133170.096554	36.868340
1686.549316	133347.712495	36.873357
1688.414916	133548.594708	36.878375
1690.149678	133720.762670	36.883392
1692.054296	133899.201916	36.888410
1693.264435	134067.476750	36.893428
1695.395866	134268.891991	36.898445
1696.861234	134429.475365	36.903463
1698.661672	134644.351402	36.908480
1700.644851	134794.515231	36.913498
1702.007606	135007.702233	36.918516
1704.110308	135154.871291	36.923533
1705.574494	135334.770540	36.928551
1707.148523	135505.821660	36.933568
1708.727616	135653.722636	36.938586
1710.287376	135815.439156	36.943604
1711.952632	135993.511247	36.948621
1713.231762	136157.428369	36.953639
1715.027350	136318.603389	36.958656
1716.386394	136489.897195	36.963674
1718.339452	136684.261511	36.968692
1720.065262	136854.498160	36.973709
1721.753880	137016.606394	36.978727
1723.126184	137213.207983	36.983744
1724.860094	137391.746576	36.988762
1726.553356	137564.907084	36.993780
1728.568236	137747.737078	36.998797
1729.984773	137946.921675	37.003815
1731.720282	138137.452475	37.008832
1733.599093	138318.115308	37.013850
1735.327731	138522.234484	37.018868
1737.212825	138711.452646	37.023885
1738.867998	138899.770749	37.028903
1740.771712	139094.982561	37.033920
1741.887942	139305.768836	37.038938
1743.713621	139499.538323	37.043956
1745.476883	139689.884606	37.048973
1747.325401	139909.936885	37.053991
1749.312670	140103.469198	37.059008
1751.430823	140297.298814	37.064026
1752.698720	140520.438650	37.069044
1754.960160	140694.579099	37.074061
1756.581031	140920.339950	37.079079
1758.564021	141098.861285	37.084096
1760.231280	141311.500566	37.089114
1762.256869	141502.513752	37.094132
1764.100414	141690.768810	37.099149
1765.759225	141874.745246	37.104167
1767.066500	142114.163888	37.109184
1769.844853	142271.919956	37.114202
1771.075689	142522.963387	37.119220
1773.020801	142695.923522	37.124237
1774.909123	142877.398112	37.129255
1777.323266	143059.715532	37.134272
1779.134014	143245.868800	37.139290
1780.465856	143494.217186	37.144308
1782.318481	143670.987213	37.149325
1784.241723	143828.937791	37.154343
1785.701524	144054.177093	37.159360
1787.753508	144212.033150	37.164378
1789.284559	144441.104446	37.169396
1791.103120	144608.239625	37.174413
1792.800350	144836.970594	37.179431
1794.895553	145030.073469	37.184448
1796.778673	145207.519237	37.189466
1798.014518	145418.506322	37.194484
1799.846315	145583.781378	37.199501
1801.892483	145794.249427	37.204519
1803.474638	145961.682925	37.209536
1805.517468	146156.816515	37.214554
1807.184135	146319.802037	37.219572
1809.026929	146495.930582	37.224589
1810.738768	146676.834349	37.229607
1812.597319	146849.032858	37.234624
1814.069998	147015.551340	37.239642
1815.607101	147214.853453	37.244660
1817.471602	147388.080723	37.249677
1819.084382	147605.639609	37.254695
1820.441542	147776.579088	37.259712
1823.102877	147976.810372	37.264730
1824.737554	148179.310184	37.269748
1826.547889	148364.036254	37.274765
1828.472869	148583.086131	37.279783
1830.239826	148762.839488	37.284800
1831.905687	148953.626008	37.289818
1833.636346	149174.168607	37.294836
1835.323664	149364.180876	37.299853
1837.950796	149535.371873	37.304871
1839.528582	149756.690679	37.309888
1841.541009	149996.298551	37.314906
1843.315720	150163.343313	37.319924
1845.168373	150387.437157	37.324941
1847.046551	150601.462635	37.329959
1848.857070	150782.678254	37.334976
1851.271215	150977.072467	37.339994
1852.743653	151222.277171	37.345012
1854.656093	151386.428539	37.350029
1856.189315	151620.330741	37.355047
1858.322563	151810.185142	37.360064
1860.265835	152024.006778	37.365082
1862.555155	152209.756420	37.370100
1864.609215	152412.317588	37.375117
1866.312954	152643.296724	37.380135
1868.210302	152812.617653	37.385152
1870.207749	153046.443634	37.390170
1872.060133	153229.326995	37.395188
1874.073524	153442.195814	37.400205
1876.099980	153617.928372	37.405223
1877.690365	153851.964102	37.410240
1879.991967	154032.003957	37.415258
1881.441350	154228.206048	37.420276
1883.257712	154449.772200	37.425293
1885.240954	154626.607315	37.430311
1887.264976	154857.234011	37.435328
1889.548158	155026.314774	37.440346
1891.072519	155251.330560	37.445364
1893.501926	155410.779226	37.450381
1894.969769	155637.645049	37.455399
1896.497326	155851.709384	37.460416
1899.367852	156008.871968	37.465434
1901.355383	156196.986694	37.470452
1903.174169	156437.064966	37.475469
1904.646148	156593.234977	37.480487
1906.661403	156760.591776	37.485504
1908.648217	156964.877543	37.490522
1909.831438	157139.938107	37.495540
1911.909877	157280.025671	37.500557
1913.733462	157481.385999	37.505575
1915.346913	157647.669704	37.510592
1917.185328	157839.684561	37.515610
1918.927632	158012.720780	37.520628
1920.802696	158230.054385	37.525645
1922.749088	158416.399906	37.530663
1924.580026	158600.025780	37.535680
1926.462003	158788.995696	37.540698
1928.216586	159004.514606	37.545716
1929.578855	159220.490209	37.550733
1931.903637	159384.856037	37.555751
1933.520749	159632.939364	37.560768
1935.510608	159836.366632	37.565786
1937.249537	160049.700680	37.570804
1939.355738	160300.640412	37.575821
1941.374047	160485.337031	37.580839
1943.529291	160680.715800	37.585856
1945.748108	160930.209167	37.590874
1947.930548	161124.888607	37.595892
1949.408688	161375.060625	37.600909
1951.410162	161576.188059	37.605927
1953.563113	161774.058793	37.610944
1955.755367	162027.406596	37.615962
1957.476683	162233.680223	37.620980
1960.075340	162423.862111	37.625997
1962.067548	162658.553161	37.631015
1963.875272	162855.850566	37.636032
1966.122847	163080.345605	37.641050
1968.476621	163283.836309	37.646068
1970.561164	163508.727664	37.651085
1972.997637	163695.809514	37.656103
1974.975348	163898.082441	37.661120
1977.058799	164114.848367	37.666138
1979.068394	164288.177205	37.671156
1980.864708	164519.918348	37.676173
1983.252261	164680.100708	37.681191
1984.842423	164911.001942	37.686208
1987.416209	165072.576930	37.691226
1989.056070	165301.608374	37.696244
1991.165424	165474.508469	37.701261
1993.182783	165692.359578	37.706279
1994.726868	165860.861420	37.711296
1996.972134	166082.229902	37.716314
1998.683770	166276.681979	37.721332
2001.266162	166444.907580	37.726349
2002.930957	166669.390267	37.731367
2004.816339	166838.819006	37.736384
2006.759549	167075.474002	37.741402
2008.859516	167237.552179	37.746420
2010.788308	167478.740007	37.751437
2013.033414	167643.587291	37.756455
2014.684084	167835.621904	37.761472
2016.475822	168024.717855	37.766490
2018.111300	168176.422395	37.771508
2020.223370	168380.131748	37.776525
2021.855057	168553.819509	37.781543
2024.187625	168736.288318	37.786560
2026.072569	168955.359025	37.791578
2028.083491	169116.660311	37.796596
2030.043832	169320.449517	37.801613
2032.363696	169527.988037	37.806631
2034.270629	169712.063842	37.811648
2036.248397	169923.172326	37.816666
2038.128537	170098.184922	37.821684
2040.130286	170327.151475	37.826701
2042.098079	170523.043450	37.831719
2044.320739	170695.366030	37.836736
2046.303471	170932.152904	37.841754
2048.463630	171120.305096	37.846772
2050.161958	171368.327695	37.851789
2052.346546	171561.856515	37.856807
2054.216171	171756.273470	37.861824
2056.401120	171993.516740	37.866842
2059.049023	172168.721309	37.871860
2061.151650	172412.652531	37.876877
2063.395268	172619.648859	37.881895
2065.719309	172851.014663	37.886912
2067.953756	173054.615067	37.891930
2070.292656	173239.958297	37.896948
2071.984656	173465.059874	37.901965
2074.647833	173628.800819	37.906983
2076.707888	173849.304754	37.912000
2078.610103	174067.665693	37.917018
2081.259360	174227.199659	37.922036
2083.050711	174455.018492	37.927053
2085.175580	174634.135367	37.932071
2087.258393	174868.316671	37.937088
2089.517926	175027.636554	37.942106
2091.424392	175257.268447	37.947124
2093.899041	175437.893793	37.952141
2096.043982	175621.084112	37.957159
2097.930518	175836.894516	37.962176
2100.357948	176018.950801	37.967194
2102.124665	176224.163829	37.972212
2104.242139	176398.164388	37.977229
2106.347950	176619.754528	37.982247
2108.842122	176783.674646	37.987264
2110.834811	177005.056453	37.992282
2113.045989	177167.335675	37.997300
2115.026947	177397.259569	38.002317
2117.590558	177548.307381	38.007335
2119.223826	177786.217822	38.012352
2121.232258	177939.194718	38.017370
2123.517721	178164.659527	38.022388
2125.671227	178328.779372	38.027405
2127.774849	178541.156694	38.032423
2129.782780	178688.249618	38.037440
2131.597005	178873.752473	38.042458
2133.898217	179008.430008	38.047476
2135.615367	179227.850079	38.052493
2138.081222	179364.583357	38.057511
2139.764595	179561.211407	38.062528
2141.638524	179724.924313	38.067546
2143.731631	179936.206537	38.072564
2145.891394	180133.675180	38.077581
2147.389100	180303.717644	38.082599
2149.728897	180481.798070	38.087616
2151.555289	180714.023031	38.092634
2154.123019	180872.986604	38.097652
2155.525513	181114.619170	38.102669
2158.369045	181292.737265	38.107687
2160.055216	181512.922599	38.112704
2162.458472	181733.997674	38.117722
2164.547080	181935.812518	38.122740
2166.779827	182147.096171	38.127757
2169.487282	182358.724272	38.132775
2171.405025	182580.578515	38.137792
2173.905513	182789.729257	38.142810
2176.627013	182984.038598	38.147828
2178.537392	183186.090512	38.152845
2180.927160	183395.756557	38.157863
2183.403554	183605.587502	38.162880
2185.422073	183805.176212	38.167898
2187.425451	184002.230487	38.172916
2189.540160	184220.521618	38.177933
2191.871706	184422.842297	38.182951
2193.690383	184620.372713	38.187968
2196.108056	184861.027457	38.192986
2199.072977	185047.693905	38.198004
2201.088703	185284.887136	38.203021
2203.311990	185471.000443	38.208039
2205.843025	185683.992092	38.213056
2208.353349	185876.761429	38.218074
2210.783663	186069.417384	38.223092
2212.729702	186295.422355	38.228109
2215.426757	186443.320438	38.233127
2217.732531	186677.302626	38.238144
2219.509954	186842.630854	38.243162
2221.992184	187058.441063	38.248180
2224.039997	187240.719141	38.253197
2226.294151	187439.195268	38.258215
2228.589423	187647.043417	38.263232
2230.726181	187836.073356	38.268250
2232.802972	188035.684182	38.273268
2235.213540	188222.210456	38.278285
2237.562402	188442.515115	38.283303
2239.864675	188625.735423	38.288320
2241.565025	188831.703581	38.293338
2244.413941	189026.919680	38.298356
2246.053774	189203.851502	38.303373
2247.907988	189426.561523	38.308391
2250.394756	189584.629774	38.313408
2252.125535	189777.094851	38.318426
2254.205400	189959.492690	38.323444
2256.246611	190148.813613	38.328461
2258.271228	190318.480459	38.333479
2260.394016	190525.061606	38.338496
2262.360805	190727.010960	38.343514
2264.642866	190927.819784	38.348532
2266.549688	191141.620704	38.353549
2268.816708	191355.365460	38.358567
2271.041782	191564.828341	38.363584
2272.946089	191786.323109	38.368602
2275.410159	192002.552261	38.373620
2277.405393	192230.900395	38.378637
2280.176498	192464.837517	38.383655
2282.249278	192692.921697	38.388672
2284.784000	192903.293070	38.393690
2286.966765	193140.524861	38.398708
2289.271807	193383.804806	38.403725
2291.861723	193604.831047	38.408743
2294.068714	193837.315805	38.413760
2296.312935	194073.260497	38.418778
2298.979825	194334.255680	38.423796
2300.796652	194546.880020	38.428813
2303.921263	194765.592929	38.433831
2306.470404	195002.737430	38.438848
2309.034139	195224.701478	38.443866
2311.956886	195436.773486	38.448884
2314.107227	195651.557969	38.453901
2316.134175	195893.840770	38.458919
2318.719891	196090.891030	38.463936
2320.896022	196312.261304	38.468954
2323.621550	196531.920854	38.473972
2325.933592	196759.363673	38.478989
2328.207555	196973.524886	38.484007
2330.783568	197195.609782	38.489024
2332.797789	197411.463968	38.494042
2335.408886	197648.458603	38.499060
2337.405407	197871.298256	38.504077
2339.907829	198085.503986	38.509095
2342.180470	198302.666281	38.514112
2344.278585	198552.476850	38.519130
2346.998558	198763.845813	38.524148
2348.763415	198991.435872	38.529165
2350.913575	199229.868816	38.534183
2353.386254	199460.242595	38.539200
2355.509642	199687.626477	38.544218
2358.060744	199922.102271	38.549236
2360.624047	200192.396469	38.554253
2362.975584	200392.178223	38.559271
2365.440358	200653.579911	38.564288
2367.408065	200871.549880	38.569306
2370.356934	201127.063691	38.574324
2372.210109	201344.761766	38.579341
2374.720992	201599.534855	38.584359
2377.314690	201787.504039	38.589376
2378.844035	202023.470964	38.594394
2381.292034	202210.385756	38.599412
2383.529353	202460.357325	38.604429
2385.771911	202645.719475	38.609447
2388.090831	202875.662402	38.614464
2390.302013	203114.293054	38.619482
2392.718069	203318.137144	38.624500
2394.656530	203581.679787	38.629517
2396.918957	203799.576472	38.634535
2399.821498	204032.782758	38.639552
2401.993283	204279.662833	38.644570
2404.344344	204531.808904	38.649588
2406.653370	204785.359082	38.654605
2408.692682	205009.909296	38.659623
2411.036013	205298.897902	38.664640
2413.196928	205526.997878	38.669658
2416.202552	205800.993839	38.674676
2418.658210	206042.847666	38.679693
2421.037147	206336.786522	38.684711
2423.838938	206580.656871	38.689728
2426.065172	206849.183076	38.694746
2428.764323	207109.041408	38.699764
2431.025873	207375.952207	38.704781
2433.659863	207633.043062	38.709799
2436.395257	207888.747934	38.714816
2438.813193	208177.738821	38.719834
2441.388635	208427.111307	38.724852
2443.946950	208688.166720	38.729869
2446.451357	208939.291753	38.734887
2449.092579	209222.704591	38.739904
2451.115441	209468.220813	38.744922
2453.911971	209726.665834	38.749940
2456.288730	210002.456410	38.754957
2458.935592	210264.532789	38.759975
2461.613291	210509.911272	38.764992
2463.808203	210804.446860	38.770010
2466.394107	211036.854768	38.775028
2468.847025	211342.955441	38.780045
2471.372386	211568.062404	38.785063
2474.302089	211865.571454	38.790080
2476.466427	212096.970951	38.795098
2479.113750	212390.172652	38.800116
2481.585649	212632.951302	38.805133
2484.019572	212909.634172	38.810151
2486.515228	213168.344066	38.815168
2488.977735	213440.543093	38.820186
2491.582304	213692.229765	38.825204
2494.082337	213970.734843	38.830221
2496.733887	214237.498792	38.835239
2499.375954	214476.283506	38.840256
2501.652739	214748.225352	38.845274
2504.015713	215016.929854	38.850292
2506.816896	215278.176875	38.855309
2508.972730	215542.015616	38.860327
2511.550878	215770.074147	38.865344
2513.662348	216004.530107	38.870362
2516.051465	216260.171005	38.875380
2518.722673	216470.378898	38.880397
2520.400922	216743.604342	38.885415
2523.147818	216969.697585	38.890432
2525.198808	217241.786733	38.895450
2527.619331	217495.725900	38.900468
2529.905769	217734.464105	38.905485
2532.558633	218031.561971	38.910503
2534.998352	218288.459259	38.915520
2536.913311	218574.719146	38.920538
2539.964330	218841.729689	38.925556
2542.465564	219134.209183	38.930573
2544.611315	219432.345489	38.935591
2547.747926	219689.162761	38.940608
2550.140291	219982.043833	38.945626
2552.823789	220290.167097	38.950644
2555.253469	220549.753073	38.955661
2557.692610	220846.883675	38.960679
2560.474594	221145.230851	38.965696
2562.656987	221490.691845	38.970714
2565.346702	221787.926148	38.975732
2568.074980	222096.735423	38.980749
2570.447955	222400.853448	38.985767
2573.622734	222691.310236	38.990784
2576.091052	223002.830805	38.995802
2578.974293	223308.192096	39.000820
2581.338533	223610.246578	39.005837
2584.272469	223900.161966	39.010855
2587.357974	224202.777421	39.015872
2589.660234	224499.080412	39.020890
2592.376122	224792.487379	39.025908
2595.208782	225091.375050	39.030925
2598.071166	225395.896946	39.035943
2600.808565	225669.469727	39.040960
2603.392531	225972.666526	39.045978
2606.048860	226274.329227	39.050996
2608.484344	226562.872904	39.056013
2611.272093	226869.773920	39.061031
2614.049485	227147.497522	39.066048
2616.306417	227445.773864	39.071066
2619.189100	227727.749266	39.076084
2621.743375	228023.415503	39.081101
2624.352659	228325.118414	39.086119
2627.538683	228621.778678	39.091136
2629.924131	228914.935063	39.096154
2632.596448	229211.323168	39.101172
2635.125396	229490.185769	39.106189
2637.670583	229793.859470	39.111207
2640.725810	230083.078701	39.116224
2643.099162	230390.565810	39.121242
2645.588795	230669.971667	39.126260
2648.527056	230969.294953	39.131277
2650.396380	231260.509024	39.136295
2652.914790	231524.014206	39.141312
2655.436948	231805.653349	39.146330
2657.904541	232070.717382	39.151348
2660.399972	232343.651022	39.156365
2663.048538	232635.761861	39.161383
2665.525948	232901.791791	39.166400
2667.839279	233193.474889	39.171418
2670.286516	233480.997798	39.176436
2672.772843	233785.582831	39.181453
2675.315654	234086.502543	39.186471
2677.994161	234391.820965	39.191488
2680.692749	234708.032996	39.196506
2683.290590	235017.658424	39.201524
2686.095232	235332.052348	39.206541
2688.190984	235651.563038	39.211559
2691.393102	235962.467157	39.216576
2694.382463	236276.555350	39.221594
2697.006418	236609.522824	39.226612
2700.086220	236923.624045	39.231629
2702.392470	237271.984816	39.236647
2705.504301	237585.244764	39.241664
2708.001203	237920.471593	39.246682
2710.724144	238243.243493	39.251700
2713.699565	238577.888575	39.256717
2716.158203	238900.094692	39.261735
2718.981654	239238.956722	39.266752
2721.843554	239577.153302	39.271770
2724.454579	239901.827303	39.276788
2727.584028	240234.827370	39.281805
2729.857106	240584.219798	39.286823
2732.658356	240917.807202	39.291840
2735.531410	241260.197903	39.296858
2737.834618	241607.912212	39.301876
2741.156024	241944.341101	39.306893
2743.640799	242295.889426	39.311911
2746.602790	242635.171147	39.316928
2749.575823	242980.954486	39.321946
2752.155891	243329.645839	39.326964
2755.613675	243668.166040	39.331981
2758.151534	244011.608094	39.336999
2760.853355	244355.507703	39.342016
2764.082923	244699.451640	39.347034
2766.315635	245041.623905	39.352052
2769.507820	245382.400467	39.357069
2772.148013	245723.138304	39.362087
2775.119218	246060.090663	39.367104
2777.853780	246417.452756	39.372122
2780.567939	246759.553080	39.377140
2783.479020	247097.863710	39.382157
2785.888254	247443.214480	39.387175
2788.995314	247794.907429	39.392192
2791.921725	248123.413228	39.397210
2794.603948	248479.340864	39.402228
2797.626425	248814.437271	39.407245
2800.325672	249151.008072	39.412263
2803.208748	249450.515378	39.417280
2806.061825	249761.179209	39.422298
2808.219640	250056.001663	39.427316
2811.075299	250370.425687	39.432333
2813.584359	250687.902586	39.437351
2815.886842	250993.245466	39.442368
2818.697630	251330.260424	39.447386
2821.123192	251653.772573	39.452404
2824.131584	251984.889763	39.457421
2826.732126	252324.886578	39.462439
2830.004054	252661.577115	39.467456
2832.576205	253007.244341	39.472474
2835.044142	253345.765395	39.477492
2838.028813	253690.174710	39.482509
2840.741702	254049.284645	39.487527
2843.735093	254413.837688	39.492544
2846.567635	254758.857282	39.497562
2849.295449	255111.895738	39.502580
2852.383368	255481.160597	39.507597
2854.804594	255852.259040	39.512615
2858.193871	256206.159953	39.517632
2860.804751	256573.470115	39.522650
2863.792976	256953.447738	39.527668
2866.924291	257312.547999	39.532685
2869.648793	257685.659185	39.537703
2872.809361	258066.348087	39.542720
2875.602412	258437.773074	39.547738
2878.515002	258803.362530	39.552756
2881.858769	259173.355127	39.557773
2884.649625	259549.659459	39.562791
2887.401551	259921.220212	39.567808
2890.682897	260291.656166	39.572826
2893.607788	260672.919830	39.577844
2897.038178	261037.414374	39.582861
2899.690197	261412.447772	39.587879
2902.464966	261784.312274	39.592896
2905.831950	262155.118177	39.597914
2908.739299	262529.071052	39.602932
2911.666707	262899.642609	39.607949
2914.586433	263263.179189	39.612967
2917.411697	263634.758467	39.617984
2920.266936	264006.079374	39.623002
2923.418606	264376.490041	39.628020
2926.372642	264745.408188	39.633037
2929.068634	265119.219537	39.638055
2932.316242	265491.064090	39.643072
2935.147148	265863.457611	39.648090
2937.892416	266245.518218	39.653108
2941.081375	266617.677893	39.658125
2943.742802	266988.625817	39.663143
2946.836545	267363.798739	39.668160
2949.829410	267744.195577	39.673178
2952.803089	268110.573135	39.678196
2956.034196	268493.930379	39.683213
2958.585435	268851.382535	39.688231
2961.661832	269202.045301	39.693248
2964.412650	269527.737534	39.698266
2966.655354	269887.118952	39.703284
2969.773707	270217.706980	39.708301
2972.330636	270581.357564	39.713319
2974.942820	270919.596205	39.718336
2977.980284	271303.544528	39.723354
2980.556238	271660.536863	39.728372
2983.130097	272035.185003	39.733389
2986.234683	272404.770195	39.738407
2989.238719	272790.934425	39.743424
2991.957275	273179.557266	39.748442
2994.903017	273564.079691	39.753460
2998.082933	273960.860376	39.758477
3001.311746	274351.307934	39.763495
3004.059393	274751.357977	39.768512
3007.407313	275145.063802	39.773530
3010.185605	275546.480828	39.778548
3013.224345	275951.692549	39.783565
3016.274876	276364.828255	39.788583
3019.349617	276773.336675	39.793600
3022.083143	277176.589735	39.798618
3025.257901	277609.774323	39.803636
3028.882960	278017.230113	39.808653
3031.991359	278439.095089	39.813671
3034.618133	278854.177250	39.818688
3037.862974	279271.854211	39.823706
3040.933336	279692.175174	39.828724
3043.856717	280118.565219	39.833741
3046.984215	280543.373152	39.838759
3050.387550	280960.694037	39.843776
3053.726280	281393.343114	39.848794
3056.469433	281813.841789	39.853812
3060.002093	282244.224141	39.858829
3062.891522	282656.316023	39.863847
3065.830715	283090.221120	39.868864
3069.365552	283511.431609	39.873882
3072.189846	283946.725957	39.878900
3075.256707	284372.988804	39.883917
3078.577997	284792.326743	39.888935
3081.573981	285229.091501	39.893952
3084.779988	285656.042378	39.898970
3087.563935	286098.479257	39.903988
3091.197880	286516.445009	39.909005
3094.388458	286942.075954	39.914023
3097.382366	287373.783425	39.919040
3100.604375	287791.508041	39.924058
3103.892481	288228.908936	39.929076
3106.813349	288650.668367	39.934093
3110.311930	289079.016762	39.939111
3113.464135	289498.960221	39.944128
3116.840154	289912.720193	39.949146
3119.713471	290333.646470	39.954164
3123.062390	290756.122622	39.959181
3125.875197	291165.524363	39.964199
3128.836365	291548.305448	39.969216
3132.027115	291931.227450	39.974234
3134.052154	292316.568734	39.979252
3137.414634	292707.159328	39.984269
3140.354276	293111.050864	39.989287
3143.060523	293496.307854	39.994304
3146.297655	293911.048548	39.999322
3148.688652	294329.046830	40.004340
3152.208324	294734.698043	40.009357
3155.294823	295161.729479	40.014375
3158.046916	295582.081374	40.019392
3161.266805	296014.119566	40.024410
3164.326507	296461.397996	40.029428
3167.248970	296888.502528	40.034445
3170.551217	297339.068213	40.039463
3173.641227	297778.387959	40.044480
3176.684755	298236.206528	40.049498
3179.610382	298695.947714	40.054516
3183.099085	299149.807036	40.059533
3186.455349	299607.572565	40.064551
3189.232893	300075.055599	40.069568
3192.870400	300534.628421	40.074586
3196.161722	301008.403294	40.079604
3199.285003	301489.823745	40.084621
3202.670812	301955.528626	40.089639
3206.134626	302418.578042	40.094656
3209.387567	302898.347918	40.099674
3212.259493	303373.502741	40.104692
3216.102194	303843.676278	40.109709
3219.863647	304309.797002	40.114727
3222.580350	304798.459526	40.119744
3226.323503	305261.862111	40.124762
3229.622191	305728.305308	40.129780
3233.001235	306206.113602	40.134797
3236.412323	306666.871447	40.139815
3239.867887	307134.402519	40.144832
3243.195029	307595.906962	40.149850
3246.591788	308070.632182	40.154868
3249.621849	308530.198996	40.159885
3253.124325	308991.187972	40.164903
3256.136156	309457.281982	40.169920
3259.745108	309933.515825	40.174938
3262.853330	310397.482742	40.179956
3266.141091	310861.216224	40.184973
3269.582490	311327.590483	40.189991
3272.473392	311805.581197	40.195008
3275.856514	312259.489771	40.200026
3278.980227	312743.256071	40.205044
3282.324536	313210.425203	40.210061
3286.106849	313676.126103	40.215079
3288.927046	314160.162669	40.220096
3292.461236	314625.568471	40.225114
3296.081310	315094.666800	40.230132
3299.513382	315557.570117	40.235149
3302.736926	316005.189131	40.240167
3305.817267	316443.964836	40.245184
3309.144277	316861.212811	40.250202
3311.840115	317291.562615	40.255220
3315.103278	317716.030083	40.260237
3318.204684	318137.778312	40.265255
3321.251789	318584.168988	40.270272
3324.635848	319017.272160	40.275290
3327.687288	319461.092848	40.280308
3330.646830	319925.624731	40.285325
3333.805092	320373.538498	40.290343
3336.678870	320847.704778	40.295360
3340.277919	321294.680778	40.300378
3343.357119	321793.063593	40.305396
3346.460974	322267.389104	40.310413
3349.868369	322738.972008	40.315431
3353.372830	323230.625486	40.320448
3356.624861	323715.001955	40.325466
3360.203351	324208.415808	40.330484
3363.624579	324702.918252	40.335501
3367.321522	325196.104360	40.340519
3370.381082	325695.737193	40.345536
3373.877603	326195.881952	40.350554
3377.482790	326704.209088	40.355572
3381.027606	327199.921165	40.360589
3384.610162	327704.537785	40.365607
3387.646577	328204.082367	40.370624
3391.479335	328712.969992	40.375642
3394.646017	329222.010352	40.380660
3397.891909	329747.439468	40.385677
3401.605091	330256.462628	40.390695
3404.920535	330772.249194	40.395712
3408.687513	331287.376703	40.400730
3411.755169	331806.420193	40.405748
3415.479595	332324.772069	40.410765
3419.123473	332837.190934	40.415783
3422.607716	333363.622892	40.420800
3426.070603	333874.818609	40.425818
3429.462797	334398.413365	40.430836
3432.921498	334914.350525	40.435853
3436.431669	335439.137561	40.440871
3440.097239	335969.228308	40.445888
3443.519164	336485.413291	40.450906
3447.080740	337010.662419	40.455924
3450.408303	337530.002787	40.460941
3454.233058	338040.043424	40.465959
3457.274655	338564.448266	40.470976
3460.998772	339087.166717	40.475994
3464.630811	339607.559527	40.481012
3468.126191	340129.696234	40.486029
3471.784992	340638.752217	40.491047
3475.212330	341164.369543	40.496064
3478.909575	341677.067130	40.501082
3482.207526	342185.355011	40.506100
3485.518602	342697.140323	40.511117
3489.014935	343201.939301	40.516122
3491.836579	343682.115384	40.521127
3495.233760	344097.493345	40.526132
3498.155688	344471.301552	40.531136
3500.560462	344787.588117	40.536141
3503.082520	345070.536101	40.541146
3504.816268	345299.061188	40.546151
3507.004706	345487.730316	40.551156
3509.168405	345632.648987	40.556160
3509.896237	345758.373656	40.561165
3511.318311	345829.748090	40.566170
3512.218362	345876.668337	40.571175
3513.456522	345891.489873	40.576180
3514.183735	345894.047510	40.581184
3514.760493	345870.616037	40.586189
3515.413846	345822.508538	40.591194
3515.718914	345774.659680	40.596199
3515.896583	345690.458577	40.601204
3516.020927	345611.432751	40.606208
3516.097717	345525.058393	40.611213
3516.492357	345413.333252	40.616218
3516.325800	345303.071083	40.621223
3516.343313	345192.448715	40.626228
3516.024810	345070.425280	40.631232
3516.034397	344947.866113	40.636237
3516.174245	344825.184286	40.641242
3515.703098	344711.991108	40.646247
3515.702271	344568.662788	40.651252
3515.691685	344436.967939	40.656256
3515.049164	344309.318004	40.661261
3514.880289	344182.407438	40.666266
3514.718932	344061.120684	40.671271
3514.461400	343941.248843	40.676276
3514.322361	343813.874606	40.681280
3513.878107	343706.580545	40.686285
3513.822106	343592.657805	40.691290
3513.447109	343476.214425	40.696295
3513.357816	343359.802017	40.701300
3512.982293	343245.420048	40.706304
3512.689339	343142.046440	40.711309
3512.728854	343023.296695	40.716314
3512.517679	342934.647759	40.721319
3512.406899	342819.917683	40.726324
3512.319173	342716.256361	40.731328
3512.163043	342600.922136	40.736333
3511.521012	342499.028055	40.741338
3511.266000	342436.476055	40.746343
3511.067843	342331.889722	40.751348
3510.978508	342240.751432	40.756352
3510.322452	342170.829846	40.761357
3510.477361	342068.172700	40.766362
3510.126489	341995.224487	40.771367
3509.923343	341921.514649	40.776372
3509.850735	341852.925927	40.781376
3509.407566	341786.864810	40.786381
3509.625842	341702.880766	40.791386
3508.968738	341652.202512	40.796391
3508.964768	341594.930006	40.801396
3509.110387	341518.949989	40.806400
3508.757298	341457.557960	40.811405
3508.882989	341404.210276	40.816410
3508.584785	341361.111497	40.821415
3508.975104	341294.969004	40.826420
3508.516677	341227.458773	40.831424
3508.292716	341198.526525	40.836429
3508.466131	341133.359980	40.841434
3508.242692	341077.801716	40.846439
3507.883830	341014.450129	40.851444
3507.657997	340992.136379	40.856448
3507.329570	340935.601840	40.861453
3507.445075	340903.357547	40.866458
3507.441588	340871.819335	40.871463
3507.421025	340823.305277	40.876468
3507.462979	340790.970734	40.881472
3507.204454	340743.206973	40.886477
3507.321323	340703.224010	40.891482
3507.169605	340676.367419	40.896487
3507.106741	340639.645630	40.901492
3507.146026	340595.602040	40.906496
3506.999862	340566.631745	40.911501
3507.364891	340515.485519	40.916506
3507.098018	340487.934306	40.921511
3506.858969	340456.662221	40.926516
3506.920004	340424.400837	40.931520
3506.539850	340397.096589	40.936525
3506.671999	340363.576626	40.941530
3506.578191	340337.194385	40.946535
3506.455214	340306.489347	40.951540
3506.580847	340277.170488	40.956544
3506.351270	340252.973375	40.961549
3506.499930	340223.421754	40.966554
3506.292435	340211.134219	40.971559
3506.557073	340173.469448	40.976564
3506.424564	340152.795243	40.981568
3506.108265	340120.109703	40.986573
3506.478879	340097.675890	40.991578
3506.352932	340070.840422	40.996583
3506.196381	340053.199174	41.001588
3506.213392	340021.479107	41.006592
3506.092324	340006.785062	41.011597
3506.205497	339985.002837	41.016602
3505.692552	339970.498010	41.021607
3506.024689	339932.007852	41.026612
3506.082583	339912.067131	41.031616
3505.675801	339889.196119	41.036621
3505.913909	339875.972591	41.041626
3505.531747	339856.126873	41.046631
3505.759763	339836.770166	41.051636
3505.657174	339830.626197	41.056640
3505.885848	339799.559856	41.061645
3505.962484	339778.317900	41.066650
3505.890222	339767.179854	41.071655
3505.847985	339743.945694	41.076660
3506.163309	339719.585870	41.081664
3505.871251	339712.555443	41.086669
3505.946498	339671.992929	41.091674
3506.009052	339667.044703	41.096679
3505.744607	339650.311343	41.101684
3505.984756	339627.694344	41.106688
3505.658192	339600.483102	41.111693
3505.613133	339591.606270	41.116698
3505.670183	339581.135049	41.121703
3505.479932	339562.888058	41.126708
3505.841251	339546.972149	41.131712
3505.544852	339529.505596	41.136717
3505.565490	339508.043303	41.141722
3505.498883	339494.638766	41.146727
3505.540351	339480.682573	41.151732
3505.634409	339468.958159	41.156736
3505.636449	339452.360809	41.161741
3505.520805	339425.039782	41.166746
3505.316544	339422.348357	41.171751
3505.371828	339396.909469	41.176756
3505.532277	339391.080254	41.181760
3505.173216	339380.343858	41.186765
3505.161123	339370.036266	41.191770
3505.101272	339353.957788	41.196775
3505.523259	339338.744994	41.201780
3505.595248	339328.322282	41.206784
3505.045896	339315.426768	41.211789
3505.214397	339294.246496	41.216794
3505.298596	339294.309589	41.221799
3504.999527	339273.330504	41.226804
3505.323839	339286.388954	41.231808
3504.977612	339269.439321	41.236813
3505.183285	339244.867549	41.241818
3505.260458	339237.931433	41.246823
3504.964147	339232.938082	41.251828
3505.459199	339210.357007	41.256832
3505.186422	339213.811232	41.261837
3505.100490	339196.922254	41.266842
3504.865494	339197.952214	41.271847
3504.932845	339179.435289	41.276852
3505.291857	339175.203832	41.281856
3505.062737	339165.439631	41.286861
3505.455837	339153.667884	41.291866
3504.926614	339151.231465	41.296871
3505.344402	339124.105995	41.301876
3505.070457	339117.989046	41.306880
3504.769293	339109.636292	41.311885
3505.114919	339099.221196	41.316890
3505.111852	339097.923474	41.321895
3505.248269	339080.617479	41.326900
3505.424371	339069.974619	41.331904
3505.264744	339067.708871	41.336909
3505.052341	339053.410882	41.341914
3505.066870	339034.902266	41.346919
3504.947636	339022.473270	41.351924
3505.385423	339010.414419	41.356928
3505.071269	339004.100169	41.361933
3505.256620	338980.702475	41.366938
3505.050613	338983.178836	41.371943
3505.174191	338962.641951	41.376948
3505.323054	338968.066000	41.381952
3505.228858	338940.384995	41.386957
3505.366259	338927.889954	41.391962
3505.279176	338916.525000	41.396967
3505.043439	338895.993984	41.401972
3505.271993	338890.943089	41.406976
3505.009476	338890.195495	41.411981
3505.481001	338870.494530	41.416986
3505.301847	338867.570009	41.421991
3505.361033	338830.547865	41.426996
3505.594797	338827.685346	41.432000
3505.253574	338821.426269	41.437005
3505.367394	338804.963816	41.442010
3504.821850	338790.082036	41.447015
3504.969762	338783.083777	41.452020
3505.108931	338762.238893	41.457024
3505.180005	338759.503913	41.462029
3505.361928	338736.259407	41.467034
3505.078867	338730.092950	41.472039
3505.127234	338729.627135	41.477044
3505.273327	338710.893980	41.482048
3504.934723	338703.819888	41.487053
3505.304357	338677.821903	41.492058
3505.293156	338683.805855	41.497063
3504.992978	338656.946423	41.502068
3505.087637	338647.461886	41.507072
3504.365866	338632.429737	41.512077
3504.988526	338628.843876	41.517082
3505.134585	338620.242167	41.522087
3504.766998	338613.605398	41.527092
3504.914385	338605.512597	41.532096
3504.857757	338602.823255	41.537101
3505.086817	338578.731194	41.542106
3504.734607	338586.601892	41.547111
3505.019650	338557.078852	41.552116
3505.052834	338555.673565	41.557120
3504.659747	338558.688636	41.562125
3504.615403	338537.389027	41.567130
3504.722685	338528.309773	41.572135
3504.981416	338538.654951	41.577140
3505.021954	338514.134461	41.582144
3504.652902	338517.909415	41.587149
3505.083361	338514.430300	41.592154
3504.817264	338498.944244	41.597159
3504.652902	338485.580406	41.602164
3504.834126	338498.050692	41.607168
3504.521532	338479.924558	41.612173
3505.001188	338463.022345	41.617178
3504.927383	338469.347141	41.622183
3504.534185	338443.546023	41.627188
3504.863136	338441.381208	41.632192
3504.789209	338453.560910	41.637197
3504.821682	338436.220262	41.642202
3504.802296	338421.840708	41.647207
3505.038601	338432.138537	41.652212
3505.148084	338407.123442	41.657216
3504.955302	338402.164572	41.662221
3505.194449	338382.322002	41.667226
3505.038826	338380.921102	41.672231
3504.832046	338374.487992	41.677236
3504.776434	338356.397566	41.682240
3504.704288	338363.358512	41.687245
3504.877662	338347.395649	41.692250
3504.608915	338330.255328	41.697255
3504.750319	338321.145194	41.702260
3505.082034	338318.572641	41.707264
3504.760912	338317.146991	41.712269
3505.059812	338300.655151	41.717274
3504.759107	338296.018807	41.722279
3504.600513	338268.245869	41.727284
3504.962720	338273.661706	41.732288
3504.568260	338280.648157	41.737293
3504.937108	338262.770622	41.742298
3504.596006	338263.893738	41.747303
3504.904258	338252.135241	41.752308
3504.868156	338234.729012	41.757312
3504.573981	338246.663554	41.762317
3504.584500	338243.683564	41.767322
3504.611529	338234.591500	41.772327
3504.444805	338208.423556	41.777332
3504.718242	338210.976891	41.782336
3504.687905	338207.519692	41.787341
3505.341246	338203.445292	41.792346
3504.581707	338193.968443	41.797351
3504.577862	338181.877430	41.802356
3504.654043	338156.282013	41.807360
3504.554422	338164.545586	41.812365
3504.642203	338166.110026	41.817370
3504.699257	338160.042484	41.822375
3504.578794	338152.628374	41.827380
3504.638079	338146.331372	41.832384
3504.522405	338141.742135	41.837389
3504.731191	338142.065552	41.842394
3504.474779	338131.440000	41.847399
3504.495742	338129.018389	41.852404
3504.592559	338122.562715	41.857408
3504.363124	338123.362707	41.862413
3504.571174	338116.609431	41.867418
3504.490861	338113.261953	41.872423
3504.556586	338109.178615	41.877428
3504.840782	338107.402707	41.882432
3504.605329	338097.155678	41.887437
3505.011655	338082.352364	41.892442
3504.840808	338086.376027	41.897447
3504.676598	338085.383776	41.902452
3504.902024	338062.386714	41.907456
3504.307907	338070.066611	41.912461
3504.761155	338064.190989	41.917466
3504.425242	338053.043413	41.922471
3504.655247	338044.530183	41.927476
3504.492962	338051.963622	41.932480
3504.300315	338044.280892	41.937485
3504.922124	338040.720590	41.942490
3504.549872	338038.004751	41.947495
3504.727061	338031.383626	41.952500
3505.022130	338033.297143	41.957504
3504.651955	338020.500325	41.962509
3504.585694	338005.313491	41.967514
3504.786099	338010.143980	41.972519
3504.725139	337993.225284	41.977524
3504.830850	337980.225947	41.982528
3504.538819	337985.134284	41.987533
3504.717061	337969.985158	41.992538
3504.562959	337954.939480	41.997543
3504.264311	337961.681712	42.002548
3504.652160	337955.969157	42.007552
3504.578086	337957.661014	42.012557
3504.513244	337944.103139	42.017562
3504.508458	337940.998274	42.022567
3504.671195	337933.590281	42.027572
3504.783848	337935.278076	42.032576
3504.414116	337926.223234	42.037581
3504.792591	337908.878661	42.042586
3504.596311	337917.412108	42.047591
3504.731262	337910.517629	42.052596
3504.761534	337888.951449	42.057600
3504.939593	337899.284027	42.062605
3504.876688	337879.641791	42.067610
3504.591112	337864.056838	42.072615
3504.452685	337861.176746	42.077620
3504.387790	337860.932480	42.082624
3504.640226	337866.951198	42.087629
3505.022251	337833.517693	42.092634
3504.732789	337824.450147	42.097639
3504.800540	337823.599417	42.102644
3505.038976	337797.901841	42.107648
3504.618772	337806.088857	42.112653
3504.552327	337806.303048	42.117658
3504.416756	337791.534422	42.122663
3504.518202	337774.284519	42.127668
3505.021250	337769.826551	42.132672
3504.522074	337770.389170	42.137677
3504.836240	337754.709381	42.142682
3504.613672	337745.733075	42.147687
3504.493596	337747.814054	42.152692
3504.841896	337747.835399	42.157696
3504.953791	337722.946943	42.162701
3504.631750	337719.764939	42.167706
3504.849064	337726.069242	42.172711
3504.474249	337710.854748	42.177716
3504.568658	337693.555024	42.182720
3504.467063	337701.029822	42.187725
3504.583747	337691.567120	42.192730
3504.447799	337686.191910	42.197735
3504.425860	337683.242482	42.202740
3504.499542	337686.005610	42.207744
3504.641644	337689.699805	42.212749
3504.598157	337664.581327	42.217754
3504.602054	337664.071621	42.222759
3504.900919	337647.630536	42.227764
3504.537725	337653.873877	42.232768
3504.334408	337639.675965	42.237773
3504.403641	337638.468610	42.242778
3504.342434	337631.376004	42.247783
3504.405009	337630.806110	42.252788
3504.629234	337636.091075	42.257792
3504.249710	337623.601134	42.262797
3504.258476	337608.784192	42.267802
3504.249641	337614.335109	42.272807
3504.529252	337618.873086	42.277812
3504.516093	337601.361236	42.282816
3504.209518	337611.923210	42.287821
3504.552755	337610.163412	42.292826
3504.497736	337600.626015	42.297831
3504.436588	337594.704389	42.302836
3504.337896	337595.891020	42.307840
3504.297262	337594.802857	42.312845
3504.569749	337595.014382	42.317850
3504.070931	337584.325236	42.322855
3504.293570	337569.958146	42.327860
3504.746150	337572.024972	42.332864
3504.418930	337584.881286	42.337869
3504.946495	337571.000576	42.342874
3504.695915	337566.661732	42.347879
3504.546228	337553.117188	42.352884
3504.640580	337544.727163	42.357888
3504.386627	337542.348991	42.362893
3504.449839	337525.690564	42.367898
3504.436290	337529.562113	42.372903
3504.369975	337522.648498	42.377908
3504.815278	337523.138180	42.382912
3504.681308	337520.435563	42.387917
3504.699409	337505.337102	42.392922
3504.481804	337495.774480	42.397927
3504.320339	337502.596898	42.402932
3504.785306	337490.304363	42.407936
3504.612292	337487.531548	42.412941
3504.569939	337466.994966	42.417946
3504.153968	337479.483486	42.422951
3504.538514	337477.513502	42.427956
3504.984685	337454.634068	42.432960
3504.744243	337454.468464	42.437965
3504.641605	337440.840091	42.442970
3504.769846	337427.098847	42.447975
3504.884866	337410.075811	42.452980
3504.730085	337417.482679	42.457984
3504.533200	337409.291416	42.462989
3504.665604	337387.352536	42.467994
3504.541949	337404.937058	42.472999
3504.517367	337396.540360	42.478004
3504.841232	337373.094735	42.483008
3504.461255	337371.372890	42.488013
3504.595878	337363.714713	42.493018
3504.435375	337373.489940	42.498023
3504.271889	337366.362562	42.503028
3504.434255	337346.913663	42.508032
3504.184273	337345.451288	42.513037
3504.666573	337335.879824	42.518042
3504.437324	337341.440152	42.523047
3504.453510	337339.324745	42.528052
3504.380237	337322.789669	42.533056
3504.367112	337317.827772	42.538061
3504.689545	337314.823887	42.543066
3504.730106	337324.923727	42.548071
3504.433352	337311.784230	42.553076
3504.408565	337309.369821	42.558080
3504.079250	337299.570266	42.563085
3504.391956	337298.069850	42.568090
3504.533365	337305.964494	42.573095
3504.288618	337317.993216	42.578100
3504.485416	337301.822744	42.583104
3504.107204	337292.387308	42.588109
3504.328869	337284.537166	42.593114
3504.158745	337282.425753	42.598119
3504.651179	337277.663952	42.603124
3504.693988	337287.508878	42.608128
3504.342037	337279.240286	42.613133
3504.208668	337266.176777	42.618138
3504.431669	337262.603110	42.623143
3504.436890	337260.718542	42.628148
3504.680099	337270.633615	42.633152
3504.403469	337263.549569	42.638157
3504.323693	337244.266201	42.643162
3504.503638	337243.550467	42.648167
3504.331249	337229.118468	42.653172
3504.531725	337240.771343	42.658176
3504.514534	337254.571515	42.663181
3504.471756	337227.747173	42.668186
3504.265310	337221.441179	42.673191
3504.693051	337215.773166	42.678196
3504.785664	337218.838799	42.683200
3504.619455	337208.275207	42.688205
3504.681419	337191.616893	42.693210
3504.654935	337186.733467	42.698215
3504.822070	337180.852085	42.703220
3504.562508	337166.179288	42.708224
3504.664026	337155.751560	42.713229
3504.623254	337155.503477	42.718234
3504.773976	337151.177535	42.723239
3504.398271	337137.312245	42.728244
3504.663543	337126.400407	42.733248
3504.550299	337131.993327	42.738253
3504.695907	337115.881815	42.743258
3504.406968	337113.585528	42.748263
3504.251149	337104.293103	42.753268
3504.580853	337098.462383	42.758272
3504.650204	337099.597002	42.763277
3504.555909	337087.189150	42.768282
3504.616706	337078.600719	42.773287
3504.181293	337070.141642	42.778292
3504.564523	337073.314079	42.783296
3504.490403	337079.486319	42.788301
3504.436086	337064.475575	42.793306
3504.328734	337054.208133	42.798311
3504.377600	337038.493744	42.803316
3504.615003	337045.864112	42.808321
3504.603975	337058.517805	42.813325
3504.447907	337033.849645	42.818330
3504.588705	337013.054860	42.823335
3504.651372	337026.206040	42.828340
3504.687740	337021.236296	42.833345
3504.360693	337002.959298	42.838349
3504.531596	336998.299219	42.843354
3504.366195	337001.634760	42.848359
3504.471864	337000.039784	42.853364
3504.899344	336985.945664	42.858369
3504.368301	336978.087195	42.863373
3504.570384	336970.291025	42.868378
3504.310816	336966.971825	42.873383
3504.110331	336969.905608	42.878388
3504.359677	336959.810872	42.883393
3504.399162	336961.459346	42.888397
3504.344458	336941.993730	42.893402
3504.232381	336939.516738	42.898407
3503.943650	336953.919943	42.903412
3504.433045	336955.650033	42.908417
3504.211807	336954.743150	42.913421
3504.337040	336948.079217	42.918426
3504.466223	336948.033375	42.923431
3504.239872	336932.820688	42.928436
3504.316158	336916.516434	42.933441
3504.408863	336925.742567	42.938445
3504.374867	336927.199005	42.943450
3504.227501	336922.741975	42.948455
3504.364649	336933.310281	42.953460
3504.353405	336907.855482	42.958465
3504.366079	336913.581254	42.963469
3504.202186	336900.140649	42.968474
3504.083278	336904.232543	42.973479
3503.939891	336909.499311	42.978484
3504.236221	336903.826590	42.983489
3503.655134	336916.977733	42.988493
3504.083692	336920.779427	42.993498
3504.119212	336935.996902	42.998503
3504.271177	336934.827368	43.003508
3504.666859	336929.215313	43.008513
3504.300339	336925.378430	43.013517
3504.645091	336905.569633	43.018522
3504.410812	336899.217094	43.023527
3504.311032	336898.901969	43.028532
3504.583702	336896.313239	43.033537
3504.087508	336891.733155	43.038541
3504.398429	336886.007212	43.043546
3504.149401	336878.689652	43.048551
3504.091379	336875.593152	43.053556
3504.555282	336870.581266	43.058561
3504.118861	336876.250754	43.063565
3504.240074	336881.348412	43.068570
3504.208587	336885.935620	43.073575
3504.442771	336881.800119	43.078580
3504.560387	336864.623793	43.083585
3504.220939	336862.615504	43.088589
3504.599194	336848.121830	43.093594
3504.512194	336864.987915	43.098599
3504.404007	336862.917611	43.103604
3504.510990	336838.538731	43.108609
3504.131573	336820.219048	43.113613
3504.034502	336822.729183	43.118618
3504.247610	336828.474190	43.123623
3504.404948	336834.915343	43.128628
3504.494607	336834.264790	43.133633
3504.207518	336841.769009	43.138637
3504.332115	336810.234016	43.143642
3504.216383	336806.993897	43.148647
3503.984051	336810.925531	43.153652
3504.421764	336809.048949	43.158657
3504.191398	336815.042261	43.163661
3504.363440	336814.327771	43.168666
3504.428034	336810.066335	43.173671
3504.514017	336806.794328	43.178676
3504.430818	336792.068111	43.183681
3504.385256	336791.515305	43.188685
3504.637249	336783.711223	43.193690
3504.242603	336786.573881	43.198695
3504.557566	336788.586117	43.203700
3504.494917	336765.405032	43.208705
3504.266975	336764.575577	43.213709
3504.375714	336751.397323	43.218714
3504.321768	336755.988090	43.223719
3504.032498	336761.125191	43.228724
3504.054566	336762.700054	43.233729
3504.293405	336761.593154	43.238733
3504.230194	336745.565476	43.243738
3504.293520	336736.925687	43.248743
3504.206705	336745.951114	43.253748
3504.483860	336723.963675	43.258753
3504.380346	336742.538000	43.263757
3504.402531	336736.374012	43.268762
3504.462404	336736.746435	43.273767
3504.239317	336715.958168	43.278772
3504.406830	336705.723590	43.283777
3504.118590	336716.231894	43.288781
3504.427640	336706.407705	43.293786
3504.620234	336714.879831	43.298791
3504.264495	336718.652782	43.303796
3504.140785	336691.586452	43.308801
3504.125244	336684.613809	43.313805
3504.083694	336681.132846	43.318810
3504.225274	336690.656765	43.323815
3504.127057	336685.453705	43.328820
3504.125830	336692.709096	43.333825
3504.070795	336693.277881	43.338829
3504.473097	336692.756099	43.343834
3504.721683	336689.483838	43.348839
3504.439739	336688.561091	43.353844
3504.526788	336662.250588	43.358849
3504.293763	336672.902912	43.363853
3504.306991	336667.707689	43.368858
3504.274235	336680.517628	43.373863
3504.353164	336669.660630	43.378868
3504.638668	336650.777566	43.383873
3504.479417	336652.355638	43.388877
3504.806319	336645.099746	43.393882
3504.911257	336640.831921	43.398887
3504.229378	336627.116753	43.403892
3504.439221	336608.194724	43.408897
3504.388571	336594.557957	43.413901
3504.295307	336597.602090	43.418906
3504.642689	336605.311515	43.423911
3504.741090	336588.265440	43.428916
3504.599542	336579.403450	43.433921
3504.374952	336589.876256	43.438925
3504.872128	336579.818654	43.443930
3504.986895	336553.096419	43.448935
3504.411141	336549.343504	43.453940
3504.504353	336547.088611	43.458945
3504.452125	336545.925894	43.463949
3504.242293	336540.969578	43.468954
3504.396014	336533.359200	43.473959
3504.448677	336527.012177	43.478964
3504.507084	336527.715771	43.483969
3504.428087	336534.347054	43.488973
3504.413949	336511.387324	43.493978
3504.282525	336493.486569	43.498983
3504.054962	336500.905045	43.503988
3504.183131	336492.942307	43.508993
3504.216453	336485.656438	43.513997
3504.124088	336498.679489	43.519002
3504.134897	336497.150411	43.524007
3504.146147	336506.924071	43.529012
3504.296251	336512.984547	43.534017
3504.000982	336502.008480	43.539021
3504.050478	336486.599342	43.544026
3504.283565	336484.755100	43.549031
3504.260978	336471.444811	43.554036
3504.220711	336477.993607	43.559041
3504.212653	336491.817949	43.564045
3504.580065	336484.301068	43.569050
3504.359815	336487.568934	43.574055
3504.381340	336477.993819	43.579060
3504.734847	336457.521629	43.584065
3504.276341	336456.957730	43.589069
3504.286822	336459.705443	43.594074
3504.505919	336455.114079	43.599079
3504.488543	336451.552912	43.604084
3504.342029	336436.352947	43.609089
3504.289020	336440.154427	43.614093
3504.356248	336427.491807	43.619098
3504.337852	336437.448361	43.624103
3504.170111	336439.918768	43.629108
3504.302221	336434.806561	43.634113
3503.991573	336442.721857	43.639117
3504.203533	336433.193001	43.644122
3504.382060	336417.610709	43.649127
3504.195750	336415.450914	43.654132
3504.410277	336405.183401	43.659137
3504.411801	336408.899891	43.664141
3504.242951	336410.530400	43.669146
3504.756594	336408.285408	43.674151
3504.412815	336397.087882	43.679156
3504.772375	336374.374510	43.684161
3504.709178	336384.159956	43.689165
3504.351511	336382.663669	43.694170
3504.300264	336348.508748	43.699175
3504.194157	336346.438099	43.704180
3504.263403	336353.402361	43.709185
3504.171920	336358.788251	43.714189
3504.142071	336349.552178	43.719194
3503.971940	336348.713578	43.724199
3503.807611	336353.576391	43.729204
3504.315023	336355.099994	43.734209
3504.272617	336362.998352	43.739213
3504.281069	336365.670019	43.744218
3504.389388	336358.168626	43.749223
3504.513108	336346.235308	43.754228
3504.676541	336331.470001	43.759233
3504.592965	336331.177768	43.764237
3504.253744	336327.565646	43.769242
3504.384047	336303.768392	43.774247
3504.356958	336289.720529	43.779252
3504.437517	336286.474811	43.784257
3504.306355	336292.121547	43.789261
3504.177949	336296.113153	43.794266
3504.235432	336310.818161	43.799271
3504.048047	336302.727087	43.804276
3504.299614	336293.675629	43.809281
3504.020587	336284.555309	43.814285
3504.208915	336266.094808	43.819290
3504.159114	336265.033530	43.824295
3503.887991	336276.073792	43.829300
3504.390970	336273.601370	43.834305
3504.330857	336290.056040	43.839309
3504.412903	336275.736353	43.844314
3503.950651	336280.849924	43.849319
3504.313925	336282.752710	43.854324
3504.342932	336281.373491	43.859329
3504.165848	336270.276875	43.864333
3504.183823	336246.548272	43.869338
3504.319265	336248.359792	43.874343
3503.961582	336259.490111	43.879348
3504.213623	336251.609589	43.884353
3504.499241	336260.907144	43.889357
3504.399406	336251.223898	43.894362
3504.133987	336262.441458	43.899367
3504.250993	336249.338169	43.904372
3504.336047	336227.940986	43.909377
3504.181040	336229.391113	43.914381
3504.263825	336231.592811	43.919386
3504.398578	336234.448173	43.924391
3504.475041	336234.257924	43.929396
3504.601093	336239.583978	43.934401
3504.361312	336210.066485	43.939405
3504.208795	336207.112177	43.944410
3504.181656	336210.782296	43.949415
3504.142850	336215.116137	43.954420
3504.531943	336199.322310	43.959425
3504.417422	336216.931158	43.964429
3504.119360	336193.176126	43.969434
3504.242542	336184.577717	43.974439
3504.047083	336187.459826	43.979444
3504.187981	336169.032253	43.984449
3504.541370	336171.420287	43.989453
3504.299682	336168.734643	43.994458
3504.540091	336171.547847	43.999463
3504.231699	336172.894939	44.004468
3504.306922	336166.391575	44.009473
3504.072393	336165.461325	44.014477
3504.074031	336154.514635	44.019482
3504.402313	336149.575049	44.024487
3504.115888	336139.692172	44.029492
3504.469046	336139.279983	44.034497
3504.353474	336147.139018	44.039501
3504.125596	336164.485775	44.044506
3504.149440	336153.917428	44.049511
3504.202188	336155.003773	44.054516
3504.296076	336138.492891	44.059521
3504.148080	336133.730425	44.064525
3504.005139	336129.501754	44.069530
3504.363606	336131.125279	44.074535
3504.141441	336129.734850	44.079540
3504.517641	336134.104918	44.084545
3504.140415	336137.041221	44.089549
3504.279154	336135.746480	44.094554
3504.427567	336105.302038	44.099559
3504.202608	336106.254087	44.104564
3504.459179	336095.292543	44.109569
3504.155085	336105.879820	44.114573
3504.241739	336111.670336	44.119578
3504.287266	336118.027406	44.124583
3504.048981	336113.966549	44.129588
3504.433676	336111.767390	44.134593
3504.103492	336090.053953	44.139597
3504.254376	336078.549061	44.144602
3504.371925	336079.116025	44.149607
3504.316559	336082.077819	44.154612
3504.430562	336072.895337	44.159617
3504.241199	336089.854170	44.164621
3504.290233	336076.405196	44.169626
3504.603434	336067.853104	44.174631
3504.219611	336049.279336	44.179636
3504.565795	336051.872169	44.184641
3504.242426	336056.378291	44.189645
3504.153901	336057.283316	44.194650
3504.319850	336054.456855	44.199655
3504.184785	336056.565713	44.204660
3504.227068	336040.113879	44.209665
3504.091099	336020.278988	44.214669
3504.152199	336031.394055	44.219674
3504.126980	336026.484887	44.224679
3504.086826	336038.532410	44.229684
3504.205450	336034.949721	44.234689
3504.291873	336030.379302	44.239693
3504.439494	336032.010704	44.244698
3504.151141	336039.540669	44.249703
3504.258587	336053.525041	44.254708
3504.528429	336038.208252	44.259713
3504.348185	336011.736094	44.264717
3503.964468	336002.454086	44.269722
3504.307698	336003.850911	44.274727
3503.976872	336006.423486	44.279732
3504.301247	335998.582413	44.284737
3504.027813	336011.863296	44.289741
3504.214806	336011.808316	44.294746
3504.378121	336019.903304	44.299751
3504.175940	335992.645441	44.304756
3504.377123	335984.951127	44.309761
3504.173174	335988.725579	44.314765
3504.216045	335986.504083	44.319770
3504.411830	335982.578253	44.324775
3504.109665	335980.793156	44.329780
3504.345935	335977.904662	44.334785
3504.333395	335987.809442	44.339789
3504.308775	335970.018948	44.344794
3504.400005	335958.167069	44.349799
3504.215334	335954.785065	44.354804
3504.119007	335953.018341	44.359809
3504.177561	335956.649470	44.364813
3504.173599	335964.898194	44.369818
3504.094656	335958.215526	44.374823
3504.349113	335962.426652	44.379828
3504.351911	335962.324419	44.384833
3504.336492	335941.935852	44.389837
3504.437845	335931.126103	44.394842
3504.565998	335923.188757	44.399847
3504.240163	335933.321272	44.404852
3504.408457	335930.723549	44.409857
3504.269742	335931.432853	44.414861
3504.483305	335910.651680	44.419866
3504.547156	335895.545622	44.424871
3504.342576	335893.974209	44.429876
3504.588741	335891.847856	44.434881
3504.299027	335888.838853	44.439885
3504.307940	335866.868081	44.444890
3504.381008	335859.219463	44.449895
3504.280283	335863.486745	44.454900
3504.644535	335860.756212	44.459905
3504.249992	335871.026883	44.464909
3504.253710	335875.201283	44.469914
3504.342615	335834.736063	44.474919
3504.229711	335831.622735	44.479924
3504.353830	335837.356438	44.484929
3504.640249	335828.426694	44.489933
3504.435019	335832.252272	44.494938
3504.252835	335830.142720	44.499943
3504.410512	335820.316874	44.504948
3504.538341	335800.898443	44.509953
3504.409553	335807.359470	44.514957
3504.325165	335801.364986	44.519962
3504.378871	335806.040628	44.524967
3503.898157	335810.775297	44.529972
3504.359801	335802.250619	44.534977
3503.891912	335786.923112	44.539981
3504.058188	335774.779310	44.544986
3504.334407	335766.182112	44.549991
3503.893137	335778.573119	44.554996
3504.010030	335777.612766	44.560001
3504.068130	335776.890821	44.565005
3504.025841	335777.050286	44.570010
3504.445438	335772.376265	44.575015
3504.228680	335781.065965	44.580020
3504.116683	335781.618305	44.585025
3503.763812	335784.830800	44.590029
3503.750586	335792.622783	44.595034
3504.127058	335793.428844	44.600039
3503.759731	335801.531375	44.605044
3504.130275	335793.046554	44.610049
3504.138929	335800.453222	44.615053
3503.867351	335799.579738	44.620058
3503.766933	335802.752323	44.625063
3504.187050	335812.410533	44.630068
3504.198774	335795.632529	44.635073
3504.069839	335801.686267	44.640077
3504.251387	335792.238500	44.645082
3504.344729	335782.855589	44.650087
3504.012131	335774.252809	44.655092
3504.314618	335775.630622	44.660097
3503.917455	335769.711038	44.665101
3504.218413	335773.405684	44.670106
3504.483180	335773.338408	44.675111
3503.951801	335786.787398	44.680116
3504.438093	335774.312978	44.685121
3504.226662	335782.492694	44.690125
3503.899030	335780.227934	44.695130
3504.150033	335780.850174	44.700135
3504.228138	335768.720309	44.705140
3504.145519	335751.855380	44.710145
3504.114741	335744.655936	44.715149
3504.117791	335749.212304	44.720154
3504.314395	335744.675362	44.725159
3504.478383	335751.751994	44.730164
3504.844694	335752.203264	44.735169
3504.407010	335750.337756	44.740173
3504.400551	335735.904661	44.745178
3504.380616	335724.248513	44.750183
3504.410028	335737.379746	44.755188
3504.267531	335728.695994	44.760193
3504.054416	335729.977118	44.765197
3503.965072	335739.053994	44.770202
3504.323206	335720.388300	44.775207
3504.257484	335709.426729	44.780212
3504.438107	335688.777980	44.785217
3504.311465	335690.096349	44.790221
3504.135609	335689.742330	44.795226
3504.156529	335691.164656	44.800231
3504.592052	335693.234238	44.805236
3504.716163	335685.119304	44.810241
3504.537226	335659.817827	44.815245
3504.102656	335667.727347	44.820250
3504.225990	335674.021244	44.825255
3504.123585	335678.314261	44.830260
3504.132910	335656.979783	44.835265
3504.233932	335681.326283	44.840269
3504.012549	335674.971590	44.845274
3504.467916	335659.574472	44.850279
3504.181891	335654.757421	44.855284
3504.197699	335641.873669	44.860289
3504.233373	335628.503088	44.865293
3504.134455	335646.415104	44.870298
3504.307596	335635.212104	44.875303
3504.099013	335637.816282	44.880308
3504.366174	335637.901370	44.885313
3504.182117	335637.370448	44.890317
3504.016335	335640.655202	44.895322
3504.388673	335617.481328	44.900327
3503.787586	335616.201704	44.905332
3504.164638	335619.909787	44.910337
3504.075230	335610.810313	44.915341
3504.052145	335612.748740	44.920346
3504.090353	335631.453710	44.925351
3503.784306	335607.827019	44.930356
3503.681624	335621.361013	44.935361
3504.041161	335624.511808	44.940365
3503.836272	335622.151267	44.945370
3504.190355	335612.141600	44.950375
3503.717625	335632.505682	44.955380
3504.288041	335612.915402	44.960385
3503.947281	335621.090125	44.965389
3504.269854	335624.170392	44.970394
3504.414067	335625.293201	44.975399
3504.377425	335629.499453	44.980404
3504.371736	335634.693638	44.985409
3504.186674	335602.290576	44.990413
3503.971332	335595.603978	44.995418
3504.368843	335589.736952	45.000423
3503.922939	335595.917188	45.005428
3504.374420	335594.598453	45.010433
3503.940120	335594.539862	45.015437
3504.218144	335592.026607	45.020442
3504.518296	335599.463586	45.025447
3504.158753	335605.222855	45.030452
3504.524542	335591.341853	45.035457
3504.118997	335587.409233	45.040461
3504.182843	335577.980043	45.045466
3504.250681	335563.764280	45.050471
3504.508100	335572.939102	45.055476
3504.400771	335567.050054	45.060481
3504.448935	335566.889734	45.065485
3504.244242	335567.380358	45.070490
3504.364110	335544.271828	45.075495
3504.209670	335550.533278	45.080500
3504.299118	335538.859807	45.085505
3504.084389	335540.064818	45.090509
3503.894707	335537.345470	45.095514
3504.318092	335535.751148	45.100519
3504.168942	335539.669706	45.105524
3504.347440	335543.663752	45.110529
3503.867949	335547.176303	45.115533
3503.908593	335544.547830	45.120538
3504.216079	335537.091231	45.125543
3504.317387	335533.282140	45.130548
3504.328291	335519.635425	45.135553
3504.070683	335519.650729	45.140557
3504.041720	335512.221858	45.145562
3504.150846	335516.099587	45.150567
3504.096882	335508.114611	45.155572
3504.561270	335512.445322	45.160577
3504.189384	335523.043407	45.165581
3504.168824	335523.046694	45.170586
3504.200566	335515.633684	45.175591
3504.061015	335504.378266	45.180596
3503.855213	335486.387173	45.185601
3504.082367	335488.489701	45.190605
3504.184250	335485.698802	45.195610
3504.012103	335490.435627	45.200615
3504.100299	335489.479807	45.205620
3504.319194	335480.153377	45.210625
3504.445720	335481.609928	45.215629
3504.241171	335490.705049	45.220634
3504.631238	335488.555935	45.225639
3504.145508	335487.028958	45.230644
3504.252641	335452.339403	45.235649
3504.047558	335461.612813	45.240653
3503.486338	335467.353062	45.245658
3503.939603	335467.739673	45.250663
3503.755144	335470.340044	45.255668
3503.916185	335467.387049	45.260673
3503.935451	335465.016524	45.265677
3504.057158	335465.582836	45.270682
3504.088850	335468.327236	45.275687
3503.868325	335478.315886	45.280692
3504.267343	335473.314154	45.285697
3504.174235	335485.573804	45.290701
3504.038339	335480.122036	45.295706
3504.004617	335485.575235	45.300711
3504.201183	335491.806659	45.305716
3504.191356	335476.177554	45.310721
3504.108830	335488.155502	45.315725
3504.116261	335491.743823	45.320730
3504.361328	335484.348001	45.325735
3504.141382	335489.677897	45.330740
3504.055932	335480.883266	45.335745
3504.074588	335469.984689	45.340749
3504.108124	335465.524421	45.345754
3504.247006	335457.712610	45.350759
3504.013062	335461.568205	45.355764
3504.240988	335454.938804	45.360769
3504.170322	335457.139329	45.365773
3504.201539	335453.672256	45.370778
3504.663171	335452.097343	45.375783
3504.044923	335462.327069	45.380788
3504.200949	335458.152922	45.385793
3504.307697	335469.413608	45.390797
3504.444474	335447.778888	45.395802
3504.517348	335426.561578	45.400807
3504.185663	335433.589317	45.405812
3504.226000	335429.535286	45.410817
3504.043691	335423.836278	45.415821
3504.139243	335430.007304	45.420826
3504.343838	335437.306664	45.425831
3504.548751	335423.960204	45.430836
3504.310063	335395.307726	45.435841
3503.686045	335400.421478	45.440845
3503.873855	335399.755395	45.445850
3504.261921	335385.514429	45.450855
3504.021092	335409.253182	45.455860
3504.369097	335390.181684	45.460865
3504.580783	335386.736993	45.465869
3504.406620	335389.488482	45.470874
3504.317019	335386.982422	45.475879
3504.109159	335373.370261	45.480884
3504.257102	335358.759934	45.485889
3503.962688	335369.804025	45.490893
3503.924676	335364.744088	45.495898
3504.096813	335354.432203	45.500903
3504.016930	335379.418383	45.505908
3504.022849	335377.737309	45.510913
3504.210983	335368.390270	45.515917
3504.110611	335362.041874	45.520922
3504.172934	335387.056485	45.525927
3504.028089	335381.300636	45.530932
3504.366806	335365.590950	45.535937
3504.172297	335375.855531	45.540941
3504.111637	335366.675108	45.545946
3504.385868	335354.157763	45.550951
3504.265881	335350.434559	45.555956
3504.426289	335352.853130	45.560961
3504.359193	335348.383305	45.565965
3504.055336	335348.533207	45.570970
3504.225637	335344.153139	45.575975
3503.768395	335356.801320	45.580980
3504.022982	335356.404710	45.585985
3504.287134	335358.526851	45.590989
3503.935124	335352.243691	45.595994
3504.167499	335334.463318	45.600999
3504.106604	335338.240649	45.606004
3504.315635	335336.298350	45.611009
3504.139602	335332.431262	45.616013
3504.260587	335334.092349	45.621018
3504.325682	335332.223719	45.626023
3504.291384	335341.699261	45.631028
3504.252377	335333.737357	45.636033
3504.546886	335331.450602	45.641037
3504.358145	335329.825757	45.646042
3504.287894	335309.343839	45.651047
3504.309508	335306.565622	45.656052
3504.243584	335300.950034	45.661057
3504.466688	335301.627604	45.666061
3504.194032	335305.540242	45.671066
3503.945682	335276.405555	45.676071
3503.828896	335274.132903	45.681076
3504.168823	335284.313010	45.686081
3504.011052	335283.650643	45.691085
3504.051608	335279.265625	45.696090
3504.108712	335263.040375	45.701095
3503.914325	335269.970053	45.706100
3504.248463	335272.539364	45.711105
3504.279100	335278.771580	45.716109
3504.055680	335276.133927	45.721114
3503.945432	335274.038442	45.726119
3504.057250	335278.246703	45.731124
3504.190867	335273.999716	45.736129
3504.107350	335272.358236	45.741133
3503.822406	335282.917157	45.746138
3504.362583	335277.638524	45.751143
3504.233682	335288.681920	45.756148
3504.571101	335280.609588	45.761153
3504.150764	335259.393824	45.766157
3504.203214	335262.822297	45.771162
3504.238867	335250.113534	45.776167
3504.074488	335250.012271	45.781172
3504.263929	335231.754970	45.786177
3504.314211	335261.150177	45.791181
3504.203273	335244.976945	45.796186
3504.448193	335237.173803	45.801191
3503.939955	335240.767286	45.806196
3503.930060	335222.719696	45.811201
3503.905101	335213.635438	45.816205
3503.764581	335228.422898	45.821210
3503.894480	335225.398444	45.826215
3503.722460	335226.163935	45.831220
3504.049355	335244.747002	45.836225
3503.827838	335248.677016	45.841229
3503.977449	335256.112375	45.846234
3504.143343	335261.559493	45.851239
3503.988168	335255.703438	45.856244
3504.096789	335240.182841	45.861249
3504.003912	335245.161724	45.866253
3504.255041	335239.292352	45.871258
3504.221504	335236.904709	45.876263
3504.040573	335241.719312	45.881268
3504.151996	335235.184678	45.886273
3504.116043	335245.907901	45.891277
3504.071297	335242.860142	45.896282
3504.087248	335246.141642	45.901287
3503.738994	335248.029655	45.906292
3503.913244	335247.747573	45.911297
3504.362519	335250.400511	45.916301
3504.063787	335237.744608	45.921306
3504.126915	335251.456121	45.926311
3504.062761	335262.692944	45.931316
3504.427465	335246.673635	45.936321
3504.302273	335230.044422	45.941325
3504.495150	335210.360967	45.946330
3504.339975	335204.504907	45.951335
3504.210499	335212.009847	45.956340
3504.499693	335203.283241	45.961345
3504.563326	335206.149889	45.966349
3503.915361	335184.537313	45.971354
3504.046268	335185.025801	45.976359
3503.953228	335184.582316	45.981364
3504.009180	335181.442263	45.986369
3504.162484	335186.433147	45.991373
3504.077395	335180.871494	45.996378
3503.983426	335184.985007	46.001383
3504.219499	335189.326374	46.006388
3504.045117	335194.929120	46.011393
3504.045898	335197.882076	46.016397
3504.175424	335191.013633	46.021402
3504.512759	335198.190205	46.026407
3503.855476	335196.995829	46.031412
3504.450119	335186.693497	46.036417
3504.428223	335174.859365	46.041421
3504.290608	335170.120647	46.046426
3504.151565	335147.383858	46.051431
3504.073363	335157.222768	46.056436
3504.255103	335156.303070	46.061441
3504.176211	335167.185836	46.066445
3503.882630	335170.669016	46.071450
3504.374772	335158.779076	46.076455
3504.448571	335161.364089	46.081460
3504.129741	335146.394733	46.086465
3504.535863	335136.300398	46.091469
3503.865499	335143.585365	46.096474
3504.511285	335130.143694	46.101479
3504.261533	335137.158510	46.106484
3504.151574	335144.074854	46.111489
3504.301126	335137.737843	46.116493
3504.295983	335130.763396	46.121498
3504.377357	335132.583494	46.126503
3504.078133	335098.619888	46.131508
3504.079968	335095.564759	46.136513
3503.943442	335112.490025	46.141517
3504.125909	335089.676933	46.146522
3504.398967	335098.467488	46.151527
3504.057083	335115.908906	46.156532
3504.267099	335080.337350	46.161537
3503.992074	335110.522311	46.166541
3504.432994	335111.343650	46.171546
3504.464139	335093.493196	46.176551
3504.021492	335102.931497	46.181556
3504.105364	335071.351216	46.186561
3504.354221	335072.075632	46.191565
3504.074246	335068.174046	46.196570
3504.265115	335080.516162	46.201575
3504.245227	335069.419956	46.206580
3504.500465	335068.666839	46.211585
3504.261320	335069.061083	46.216589
3504.199938	335060.975398	46.221594
3504.279929	335045.357454	46.226599
3504.412908	335042.077932	46.231604
3504.181123	335036.361256	46.236609
3504.060910	335034.241882	46.241613
3503.950309	335040.241874	46.246618
3504.407065	335041.009796	46.251623
3504.328484	335037.560060	46.256628
3504.118381	335038.687976	46.261633
3503.873730	335034.195286	46.266637
3504.001356	335035.244354	46.271642
3504.372294	335017.340165	46.276647
3504.071323	335018.787934	46.281652
3504.299056	335011.191142	46.286657
3504.556041	335012.830737	46.291661
3504.343451	335017.726732	46.296666
3504.422178	335012.215540	46.301671
3504.144607	335022.315103	46.306676
3504.067550	335002.063285	46.311681
3504.064294	334991.600870	46.316685
3503.633683	334982.173392	46.321690
3504.349900	334992.446801	46.326695
3504.163583	334983.998997	46.331700
3504.148828	334986.547101	46.336705
3504.167716	334991.050102	46.341709
3504.240191	334989.969473	46.346714
3504.318363	334987.818736	46.351719
3504.473650	334989.805354	46.356724
3504.504082	334981.857890	46.361729
3504.366467	334961.997493	46.366733
3504.399302	334960.490355	46.371738
3504.536692	334951.787715	46.376743
3504.014212	334958.056486	46.381748
3503.731773	334959.781358	46.386753
3504.103109	334957.024213	46.391757
3503.982741	334968.371800	46.396762
3504.004997	334966.509932	46.401767
3503.951265	334966.365719	46.406772
3504.073325	334956.316264	46.411777
3504.062831	334968.792062	46.416781
3503.957972	334961.680618	46.421786
3504.221322	334956.827583	46.426791
3504.235853	334968.561162	46.431796
3504.113156	334951.931487	46.436801
3504.065852	334935.748122	46.441805
3504.111646	334924.055990	46.446810
3503.826841	334926.214012	46.451815
3504.046714	334937.456902	46.456820
3504.213629	334936.946863	46.461825
3504.201210	334923.354631	46.466829
3503.975816	334932.529493	46.471834
3504.282183	334925.505780	46.476839
3504.163256	334927.739409	46.481844
3504.114553	334926.907052	46.486849
3504.062329	334935.188988	46.491853
3504.005459	334934.128806	46.496858
3504.056177	334930.098562	46.501863
3503.944925	334936.455070	46.506868
3504.028470	334929.313838	46.511873
3503.970378	334934.516361	46.516877
3503.727512	334934.249304	46.521882
3504.376251	334939.645574	46.526887
3504.039105	334942.346475	46.531892
3504.124100	334934.899526	46.536897
3503.929318	334921.005177	46.541901
3503.835487	334916.717752	46.546906
3503.899666	334917.496822	46.551911
3503.896905	334927.705699	46.556916
3504.067735	334913.702636	46.561921
3503.754670	334927.804631	46.566925
3503.704278	334925.750588	46.571930
3504.064171	334932.770878	46.576935
3503.997126	334935.785483	46.581940
3503.441234	334943.536064	46.586945
3503.727386	334954.539357	46.591949
3503.698684	334955.536769	46.596954
3504.031123	334953.116718	46.601959
3503.985987	334968.932906	46.606964
3504.018582	334963.378088	46.611969
3504.180804	334965.567270	46.616973
3504.039350	334965.386010	46.621978
3504.037295	334959.403894	46.626983
3503.899304	334969.099539	46.631988
3504.132120	334970.182895	46.636993
3504.328228	334967.657110	46.641997
3504.045350	334962.483109	46.647002
3504.212227	334952.579312	46.652007
3503.970230	334956.665324	46.657012
3504.148185	334946.988892	46.662017
3504.281420	334945.211308	46.667021
3503.968623	334951.345103	46.672026
3504.045510	334947.361637	46.677031
3503.976667	334950.580184	46.682036
3504.258514	334943.534892	46.687041
3504.587337	334954.786013	46.692045
3504.153713	334940.471193	46.697050
3504.432022	334927.443979	46.702055
3503.795788	334923.344130	46.707060
3503.892403	334917.193669	46.712065
3504.240781	334924.648555	46.717069
3503.848534	334920.102818	46.722074
3503.822097	334913.259002	46.727079
3504.011772	334919.847970	46.732084
3504.053593	334922.998109	46.737089
3504.180867	334922.061561	46.742093
3504.076215	334936.690669	46.747098
3504.596142	334926.807428	46.752103
3504.330111	334925.092963	46.757108
3504.221480	334927.477708	46.762113
3504.254235	334933.022272	46.767117
3504.015057	334923.386321	46.772122
3503.906627	334895.222190	46.777127
3503.827374	334895.311128	46.782132
3504.321617	334918.042838	46.787137
3504.318898	334904.245409	46.792141
3504.172121	334896.376864	46.797146
3504.189084	334894.974063	46.802151
3504.057402	334903.930456	46.807156
3504.062313	334896.216133	46.812161
3504.490721	334897.090367	46.817165
3504.514141	334900.396161	46.822170
3504.570337	334880.505101	46.827175
3504.352634	334863.534021	46.832180
3504.481912	334851.370446	46.837185
3504.629339	334859.595372	46.842189
3503.950493	334866.499847	46.847194
3504.271258	334863.496119	46.852199
3504.534225	334866.153068	46.857204
3504.320488	334843.173412	46.862209
3504.155092	334830.750928	46.867213
3504.244532	334825.390771	46.872218
3504.228941	334831.095731	46.877223
3504.226033	334823.255348	46.882228
3504.218895	334836.316160	46.887233
3504.102631	334838.294797	46.892237
3503.783155	334840.687419	46.897242
3504.185798	334833.342988	46.902247
3504.140829	334843.864039	46.907252
3504.142946	334828.411101	46.912257
3504.188480	334805.772306	46.917261
3503.621500	334799.446707	46.922266
3503.807437	334792.798423	46.927271
3503.908563	334796.193767	46.932276
3503.840195	334803.103570	46.937281
3504.200067	334798.184351	46.942285
3503.849508	334809.237408	46.947290
3504.105589	334801.534282	46.952295
3503.936766	334806.907064	46.957300
3503.918096	334807.826519	46.962305
3504.021142	334810.203262	46.967309
3504.068537	334813.097951	46.972314
3504.280743	334813.904536	46.977319
3504.358294	334815.216099	46.982324
3504.458000	334804.380975	46.987329
3504.397018	334821.523488	46.992333
3504.045513	334816.996760	46.997338
3504.482428	334806.872051	47.002343
3503.888792	334788.636596	47.007348
3503.886812	334786.320321	47.012353
3504.002331	334784.290961	47.017357
3503.668072	334785.769455	47.022362
3503.997621	334777.647393	47.027367
3503.984656	334788.825286	47.032372
3503.882890	334779.549454	47.037377
3504.000207	334777.316149	47.042381
3503.749956	334789.498936	47.047386
3503.990107	334805.931955	47.052391
3503.928754	334816.073739	47.057396
3503.957896	334811.970527	47.062401
3504.165061	334800.252863	47.067405
3504.212481	334801.849220	47.072410
3504.398918	334797.593854	47.077415
3504.148103	334794.247705	47.082420
3504.114423	334785.775747	47.087425
3504.315584	334801.425751	47.092429
3504.124038	334806.573008	47.097434
3504.350603	334794.444958	47.102439
3504.289360	334795.600260	47.107444
3504.000319	334776.451098	47.112449
3504.066061	334769.821813	47.117453
3504.052835	334757.451632	47.122458
3504.135431	334755.529305	47.127463
3504.187661	334764.329355	47.132468
3504.014532	334764.254931	47.137473
3504.163341	334774.796275	47.142477
3504.037129	334776.725571	47.147482
3504.541583	334761.931470	47.152487
3504.540264	334773.107525	47.157492
3504.559836	334764.601688	47.162497
3504.060281	334727.945624	47.167501
3504.388965	334747.597755	47.172506
3504.103286	334740.998564	47.177511
3504.180483	334737.804218	47.182516
3504.219275	334728.531616	47.187521
3504.529269	334734.286943	47.192525
3504.090067	334741.026260	47.197530
3503.956083	334733.308418	47.202535
3504.146721	334740.330027	47.207540
3503.874489	334727.848041	47.212545
3504.222745	334731.077034	47.217549
3504.348872	334724.947347	47.222554
3504.250832	334698.054364	47.227559
3504.130346	334707.059927	47.232564
3504.062120	334709.972898	47.237569
3504.394614	334701.799447	47.242573
3504.008804	334707.664774	47.247578
3504.374276	334703.712045	47.252583
3504.477007	334703.415810	47.257588
3504.466802	334689.619522	47.262593
3504.206766	334676.931940	47.267597
3504.047420	334667.945227	47.272602
3504.045701	334671.535038	47.277607
3504.094109	334682.346842	47.282612
3503.804389	334670.529504	47.287617
3504.245509	334678.606193	47.292621
3503.577945	334690.473107	47.297626
3504.146577	334676.101619	47.302631
3504.153139	334680.377471	47.307636
3503.927888	334677.994659	47.312641
3504.391038	334680.416309	47.317645
3503.998367	334682.184072	47.322650
3504.187055	334671.996754	47.327655
3503.938959	334685.324804	47.332660
3503.850771	334683.200357	47.337665
3504.062295	334666.135915	47.342669
3504.165909	334683.405186	47.347674
3504.101792	334656.150420	47.352679
3503.989002	334643.414096	47.357684
3503.813466	334655.177776	47.362689
3503.896196	334653.051765	47.367693
3503.634527	334671.193424	47.372698
3504.017004	334661.637364	47.377703
3503.778256	334700.497764	47.382708
3503.864258	334691.523183	47.387713
3504.108219	334685.171204	47.392717
3503.996186	334704.052924	47.397722
3504.125497	334699.399263	47.402727
3504.312156	334681.575032	47.407732
3503.853399	334659.346858	47.412737
3504.272438	334652.992657	47.417741
3503.821962	334676.815720	47.422746
3504.079189	334656.663699	47.427751
3504.196746	334653.437511	47.432756
3503.728411	334660.843335	47.437761
3503.825021	334665.410443	47.442765
3503.997767	334676.228049	47.447770
3504.388277	334657.022341	47.452775
3504.504443	334657.793195	47.457780
3504.121464	334670.709794	47.462785
3504.613711	334660.550859	47.467789
3504.328149	334658.814017	47.472794
3504.007060	334653.569661	47.477799
3504.427086	334631.228012	47.482804
3503.912409	334632.607743	47.487809
3504.375588	334630.574333	47.492813
3504.030217	334626.835804	47.497818
3503.949834	334644.388747	47.502823
3504.310832	334637.763688	47.507828
3504.222135	334639.559770	47.512833
3504.275521	334632.117786	47.517837
3503.825653	334626.664669	47.522842
3504.346605	334642.951506	47.527847
3504.382564	334593.863839	47.532852
3504.188493	334600.946279	47.537857
3504.331601	334623.275362	47.542861
3503.832905	334595.401920	47.547866
3504.049841	334607.943660	47.552871
3504.121035	334599.353270	47.557876
3504.250757	334590.295392	47.562881
3504.533339	334607.969167	47.567885
3504.508973	334604.918158	47.572890
3504.358067	334582.514005	47.577895
3504.379835	334573.829595	47.582900
3504.077021	334585.002427	47.587905
3504.187406	334579.409823	47.592909
3504.182486	334581.549068	47.597914
3503.988999	334573.255092	47.602919
3504.042750	334565.889415	47.607924
3504.106815	334571.250856	47.612929
3503.998294	334582.291144	47.617933
3504.142561	334582.701152	47.622938
3504.179697	334574.676208	47.627943
3504.182557	334580.149154	47.632948
3503.765639	334578.331245	47.637953
3504.141138	334549.734065	47.642957
3503.820918	334541.281917	47.647962
3503.810172	334546.578815	47.652967
3503.824295	334554.519360	47.657972
3503.941751	334576.648853	47.662977
3504.281693	334581.763021	47.667981
3503.870349	334559.527319	47.672986
3504.148758	334548.867565	47.677991
3504.112045	334543.730990	47.682996
3503.733049	334563.215015	47.688001
3504.037631	334546.925016	47.693005
3503.659576	334547.341223	47.698010
3503.972518	334549.888454	47.703015
3503.835909	334564.420863	47.708020
3504.019992	334546.087855	47.713025
3504.161436	334570.937510	47.718029
3503.944011	334547.245528	47.723034
3504.128772	334562.541774	47.728039
3504.107321	334558.853864	47.733044
3503.711958	334550.209937	47.738049
3504.125837	334541.590824	47.743053
3503.794893	334560.099869	47.748058
3504.243377	334558.908877	47.753063
3504.159771	334555.510825	47.758068
3504.028426	334551.356596	47.763073
3504.328231	334555.535184	47.768077
3503.993548	334575.928671	47.773082
3504.119905	334562.518089	47.778087
3504.122719	334559.870101	47.783092
3503.919919	334563.797196	47.788097
3504.177978	334558.766767	47.793101
3504.268636	334567.942630	47.798106
3503.945089	334559.491010	47.803111
3504.045800	334560.366139	47.808116
3504.290652	334565.266223	47.813121
3504.274229	334533.166943	47.818125
3503.767476	334541.444409	47.823130
3504.216194	334529.815801	47.828135
3504.103913	334528.280680	47.833140
3504.077244	334538.798884	47.838145
3504.140713	334533.722844	47.843149
3503.963080	334537.951451	47.848154
3504.261369	334522.375251	47.853159
3504.199866	334545.347685	47.858164
3504.303727	334535.148300	47.863169
3503.930558	334548.954384	47.868173
3503.572161	334545.421570	47.873178
3503.959586	334539.708794	47.878183
3504.160276	334551.031152	47.883188
3504.081620	334541.395229	47.888193
3504.412303	334547.936484	47.893197
3504.062117	334522.508914	47.898202
3504.255939	334520.925402	47.903207
3504.126361	334488.258466	47.908212
3504.020798	334527.581602	47.913217
3504.113909	334502.796756	47.918221
3504.034895	334514.494285	47.923226
3504.277600	334511.935660	47.928231
3503.917085	334514.131121	47.933236
3503.776502	334525.863839	47.938241
3503.798661	334526.038575	47.943245
3503.650268	334516.210013	47.948250
3503.892040	334518.844869	47.953255
3503.927723	334526.883839	47.958260
3504.118386	334530.086839	47.963265
3504.115776	334522.424578	47.968269
3503.847801	334523.027043	47.973274
3504.235315	334526.631702	47.978279
3504.195342	334521.393810	47.983284
3504.228689	334527.931156	47.988289
3504.538287	334535.544961	47.993293
3504.131984	334518.272663	47.998298
3504.082836	334514.334555	48.003303
3504.153206	334494.390228	48.008308
3503.782277	334499.133088	48.013313
3504.160817	334491.130536	48.018317
3503.880533	334504.081846	48.023322
3504.022577	334495.887564	48.028327
3503.607151	334500.001020	48.033332
3503.942231	334497.987856	48.038337
3504.038665	334488.960685	48.043341
3503.784112	334505.141033	48.048346
3504.285621	334495.438845	48.053351
3503.901424	334491.299127	48.058356
3503.865925	334498.814745	48.063361
3503.849540	334496.271620	48.068365
3503.934879	334499.644017	48.073370
3504.056653	334495.067907	48.078375
3503.947069	334500.787753	48.083380
3503.871433	334499.806903	48.088385
3504.181401	334494.259114	48.093389
3504.059524	334504.741460	48.098394
3504.209824	334501.051854	48.103399
3504.059124	334502.908656	48.108404
3503.790279	334509.239201	48.113409
3504.023351	334514.344811	48.118413
3503.885343	334524.065979	48.123418
3503.915333	334509.855981	48.128423
3503.773280	334514.995436	48.133428
3504.037422	334515.870186	48.138433
3504.185020	334510.602642	48.143437
3503.880114	334516.124246	48.148442
3504.424771	334507.204422	48.153447
3504.303554	334516.057381	48.158452
3503.930499	334520.240510	48.163457
3504.160605	334518.498517	48.168461
3504.050962	334520.527031	48.173466
3504.169631	334509.943438	48.178471
3504.199193	334505.203703	48.183476
3504.157434	334500.780733	48.188481
3504.013994	334491.638738	48.193485
3503.920706	334490.940712	48.198490
3503.975259	334488.029967	48.203495
3503.872040	334482.216547	48.208500
3503.832121	334496.428195	48.213505
3504.086400	334494.606007	48.218509
3504.347564	334490.542469	48.223514
3504.886308	334485.544035	48.228519
3504.528451	334490.641235	48.233524
3503.997903	334492.125308	48.238529
3504.161057	334471.478954	48.243533
3503.860003	334473.054036	48.248538
3504.303877	334456.792910	48.253543
3504.395556	334457.491265	48.258548
3504.099286	334462.527815	48.263553
3504.092350	334447.559916	48.268557
3504.171665	334478.962014	48.273562
3504.327316	334453.301707	48.278567
3504.226218	334463.806232	48.283572
3504.150943	334468.578728	48.288577
3504.393421	334460.063073	48.293581
3504.233534	334450.007201	48.298586
3504.289024	334436.225935	48.303591
3504.600492	334435.336634	48.308596
3504.389915	334432.773291	48.313601
3504.479379	334410.992978	48.318605
3504.233640	334445.323182	48.323610
3504.276837	334385.898460	48.328615
3504.033871	334413.507444	48.333620
3504.477078	334392.587676	48.338625
3504.401875	334386.540701	48.343629
3504.107693	334397.864944	48.348634
3504.357124	334392.046683	48.353639
3504.033809	334396.476533	48.358644
3504.167737	334398.059224	48.363649
3504.074415	334397.412118	48.368653
3504.027350	334372.674842	48.373658
3504.190151	334355.083417	48.378663
3504.029541	334353.683220	48.383668
3504.256496	334350.414267	48.388673
3504.319902	334352.364514	48.393677
3504.047717	334358.084619	48.398682
3504.301248	334351.094658	48.403687
3504.480127	334357.659929	48.408692
3504.463709	334355.167719	48.413697
3504.390102	334341.661418	48.418701
3504.306299	334332.891838	48.423706
3504.289427	334315.965246	48.428711
3504.169046	334321.661356	48.433716
3504.068435	334328.907253	48.438721
3504.208400	334325.753881	48.443725
3504.281690	334327.218872	48.448730
3504.332828	334320.031785	48.453735
3504.332945	334307.608499	48.458740
3504.191513	334299.204431	48.463745
3504.304297	334280.526218	48.468749
3504.106932	334285.037993	48.473754
3504.396718	334277.304023	48.478759
3504.676947	334293.501710	48.483764
3504.300833	334274.595292	48.488769
3504.352051	334272.957945	48.493773
3504.423262	334254.260840	48.498778
3504.221566	334254.623711	48.503783
3504.392055	334261.928588	48.508788
3504.309529	334251.224017	48.513793
3504.384799	334247.800835	48.518797
3504.386352	334249.582659	48.523802
3504.292303	334230.504351	48.528807
3504.264311	334214.674170	48.533812
3504.081470	334229.315789	48.538817
3504.337596	334199.489912	48.543821
3504.153978	334220.979758	48.548826
3504.213800	334226.469184	48.553831
3504.389540	334216.996661	48.558836
3504.261379	334211.798145	48.563841
3504.331674	334193.228455	48.568845
3503.916462	334197.647387	48.573850
3503.977884	334182.439505	48.578855
3504.043217	334182.098265	48.583860
3503.851369	334187.703853	48.588865
3503.930184	334191.510076	48.593869
3503.813777	334197.485602	48.598874
3504.337118	334186.837988	48.603879
3504.058035	334176.546342	48.608884
3504.070886	334190.826083	48.613889
3504.057677	334191.031869	48.618893
3503.784771	334205.407697	48.623898
3503.984116	334186.002960	48.628903
3504.260172	334186.468510	48.633908
3503.949650	334191.049095	48.638913
3503.929808	334190.594032	48.643917
3504.364427	334200.326551	48.648922
3504.135278	334196.289592	48.653927
3504.314732	334211.434008	48.658932
3503.919790	334179.470776	48.663937
3504.021600	334167.336880	48.668941
3503.936567	334161.062322	48.673946
3504.231070	334161.932277	48.678951
3504.188316	334167.208806	48.683956
3503.965964	334169.255147	48.688961
3504.202774	334157.354485	48.693965
3504.367718	334160.459737	48.698970
3504.245758	334166.028822	48.703975
3504.196710	334164.458238	48.708980
3504.424279	334161.520128	48.713985
3504.324193	334154.738796	48.718989
3503.872697	334144.194367	48.723994
3504.353032	334126.247195	48.728999
3503.934727	334122.749288	48.734004
3504.019726	334132.307968	48.739009
3504.133816	334129.922407	48.744013
3504.325248	334119.989152	48.749018
3504.029815	334121.868844	48.754023
3504.070971	334127.284857	48.759028
3503.943844	334131.861912	48.764033
3504.295162	334127.300405	48.769037
3504.065450	334143.018672	48.774042
3503.982412	334131.830468	48.779047
3504.394316	334129.983353	48.784052
3503.992321	334128.239446	48.789057
3504.088863	334097.624108	48.794061
3504.207344	334103.078814	48.799066
3504.315649	334087.405262	48.804071
3503.864851	334094.706543	48.809076
3503.912960	334092.738734	48.814081
3504.268630	334089.143928	48.819085
3504.158823	334088.270306	48.824090
3503.964067	334088.199300	48.829095
3504.035064	334096.920095	48.834100
3504.045734	334098.751398	48.839105
3504.043007	334093.787620	48.844109
3504.160908	334098.860553	48.849114
3504.294075	334104.745717	48.854119
3504.310362	334097.436829	48.859124
3503.965760	334103.244776	48.864129
3504.344372	334089.463275	48.869133
3504.198772	334094.934271	48.874138
3504.208085	334078.028940	48.879143
3504.326776	334071.823998	48.884148
3504.173589	334087.530181	48.889153
3504.039127	334076.757420	48.894157
3504.130288	334075.088297	48.899162
3504.425300	334079.598621	48.904167
3504.398408	334083.523391	48.909172
3504.049639	334070.442402	48.914177
3503.847432	334045.118551	48.919181
3503.821065	334050.137921	48.924186
3503.553579	334055.042663	48.929191
3503.950959	334078.350031	48.934196
3504.019515	334088.878708	48.939201
3504.050522	334066.827494	48.944205
3504.312808	334086.897633	48.949210
3504.009825	334063.040808	48.954215
3503.965307	334050.828194	48.959220
3503.953148	334050.702864	48.964225
3504.172319	334052.297546	48.969229
3503.981693	334054.160671	48.974234
3504.001928	334045.909219	48.979239
3504.389286	334042.818555	48.984244
3504.092560	334049.179007	48.989249
3504.437664	334048.360757	48.994253
3504.145159	334057.775464	48.999258
3504.359751	334052.446379	49.004263
3504.441678	334043.345069	49.009268
3503.946949	334029.625247	49.014273
3504.190893	334015.737732	49.019277
3504.239889	334025.658526	49.024282
3504.046469	334017.262642	49.029287
3504.438743	334023.106852	49.034292
3503.885532	334017.975516	49.039297
3504.190587	334012.937619	49.044301
3504.237852	334022.960518	49.049306
3504.425368	334024.000134	49.054311
3504.276160	334014.146172	49.059316
3503.953123	333999.253605	49.064321
3504.350777	333983.712492	49.069325
3504.161928	333973.432009	49.074330
3503.854821	333982.288964	49.079335
3504.152017	333988.530074	49.084340
3504.026355	333987.735329	49.089345
3504.189077	333979.715921	49.094349
3503.860717	333979.818783	49.099354
3503.953483	333984.539289	49.104359
3503.684022	333986.134845	49.109364
3503.696552	333988.296806	49.114369
3503.954943	333985.913886	49.119373
3503.894225	333995.724740	49.124378
3504.122297	333999.583751	49.129383
3504.553329	333988.288799	49.134388
3504.110588	333987.162315	49.139393
3504.229257	333989.180209	49.144397
3504.098551	333989.099078	49.149402
3504.172542	333995.171810	49.154407
3504.128288	333990.749202	49.159412
3504.278684	333987.543250	49.164417
3504.221495	333961.763662	49.169421
3503.844029	333971.370016	49.174426
3504.014144	333969.790239	49.179431
3504.071454	333972.785227	49.184436
3503.841318	333967.093659	49.189441
3503.999737	333960.551476	49.194445
3503.783578	333972.118032	49.199450
3504.123056	333969.111307	49.204455
3504.215541	333958.506312	49.209460
3504.121219	333973.235821	49.214465
3504.395935	333965.020502	49.219469
3504.113152	333973.568121	49.224474
3503.994351	333979.391298	49.229479
3504.105505	333973.263912	49.234484
3504.123804	333971.097150	49.239489
3504.081066	333971.307605	49.244493
3503.955208	333977.742883	49.249498
3504.195563	333960.470049	49.254503
3504.110988	333942.790338	49.259508
3503.803877	333939.682167	49.264513
3504.037759	333930.327702	49.269517
3504.104789	333927.414961	49.274522
3504.012299	333929.288034	49.279527
3504.202617	333939.313787	49.284532
3504.178360	333934.837099	49.289537
3504.215647	333929.103252	49.294541
3504.072892	333932.155327	49.299546
3504.352049	333941.785170	49.304551
3504.260617	333931.972978	49.309556
3504.093736	333940.705940	49.314561
3504.353425	333928.165178	49.319565
3503.836629	333913.226850	49.324570
3503.768105	333913.441382	49.329575
3503.888560	333929.766242	49.334580
3504.046253	333940.077188	49.339585
3504.100735	333935.384391	49.344589
3503.906967	333944.528926	49.349594
3503.910189	333922.991214	49.354599
3504.484016	333907.676811	49.359604
3504.304935	333904.650229	49.364609
3504.479944	333905.106297	49.369613
3504.112292	333904.884420	49.374618
3504.199576	333900.899251	49.379623
3504.212989	333908.025335	49.384628
3504.060580	333914.362985	49.389633
3504.277540	333905.443973	49.394637
3504.034940	333907.926304	49.399642
3504.148967	333877.282648	49.404647
3503.881770	333873.557178	49.409652
3503.830530	333874.049013	49.414657
3503.813397	333883.980281	49.419661
3503.734002	333880.505158	49.424666
3503.733241	333895.245351	49.429671
3503.883426	333908.739706	49.434676
3503.724884	333919.329768	49.439681
3503.962673	333917.917496	49.444685
3503.675219	333910.860267	49.449690
3503.724185	333930.276815	49.454695
3504.264349	333916.189706	49.459700
3503.898349	333922.917529	49.464705
3503.945815	333904.911442	49.469709
3504.227601	333921.898159	49.474714
3504.015353	333930.689210	49.479719
3503.910264	333925.817975	49.484724
3503.892124	333922.154966	49.489729
3504.052711	333927.450283	49.494733
3504.336845	333921.346462	49.499738
3503.957498	333906.080911	49.504743
3504.080326	333892.976251	49.509748
3504.142295	333895.843217	49.514753
3504.096141	333879.175726	49.519757
3503.978849	333888.384552	49.524762
3504.112671	333878.154877	49.529767
3504.199127	333886.134980	49.534772
3504.012417	333892.147103	49.539777
3504.508577	333876.055781	49.544781
3504.256200	333890.199308	49.549786
3504.096179	333897.989254	49.554791
3504.088054	333894.273745	49.559796
3504.019724	333897.975957	49.564801
3504.180664	333887.614707	49.569805
3503.851392	333869.566337	49.574810
3504.384768	333875.846493	49.579815
3504.104304	333865.758682	49.584820
3503.655300	333876.012802	49.589825
3504.534083	333852.936478	49.594829
3504.262676	333869.450589	49.599834
3504.596538	333860.462175	49.604839
3504.516282	333861.442294	49.609844
3504.302957	333846.659639	49.614849
3504.319013	333839.070725	49.619853
3503.814724	333849.919117	49.624858
3503.968715	333826.142715	49.629863
3504.040799	333826.284103	49.634868
3503.907820	333825.235936	49.639873
3503.943683	333821.029772	49.644877
3503.997380	333829.498758	49.649882
3503.850945	333833.086031	49.654887
3503.875529	333823.917386	49.659892
3503.634134	333830.243653	49.664897
3503.927275	333825.614950	49.669901
3503.602075	333828.492209	49.674906
3504.113299	333846.282780	49.679911
3504.047666	333852.199393	49.684916
3503.891392	333854.311671	49.689921
3503.843029	333827.130462	49.694925
3503.925473	333838.038848	49.699930
3503.768540	333856.902437	49.704935
3504.209057	333862.739034	49.709940
3504.152166	333849.739150	49.714945
3504.044141	333828.524489	49.719949
3503.679964	333848.871936	49.724954
3504.142267	333838.081171	49.729959
3504.059057	333815.182371	49.734964
3503.797031	333847.096955	49.739969
3504.408441	333823.986517	49.744973
3503.711346	333859.177553	49.749978
3504.010768	333840.622464	49.754983
3504.147396	333833.701847	49.759988
3504.208794	333834.914151	49.764993
3504.014022	333842.429562	49.769997
3504.171702	333834.487307	49.775002
3503.909075	333826.356918	49.780007
3504.113432	333849.134807	49.785012
3503.639840	333829.225367	49.790017
3504.491350	333842.430662	49.795021
3504.141018	333844.319040	49.800026
3503.957430	333851.272611	49.805031
3504.415906	333843.130059	49.810036
3504.041932	333845.556788	49.815041
3504.127690	333818.048880	49.820045
3503.906297	333813.603348	49.825050
3503.779228	333814.310833	49.830055
3504.260700	333802.829672	49.835060
3503.980812	333813.922630	49.840065
3504.127758	333814.052184	49.845069
3504.034441	333810.248307	49.850074
3503.812703	333822.706791	49.855079
3504.005331	333810.329356	49.860084
3504.038770	333812.946258	49.865089
3503.917365	333805.073577	49.870093
3503.967822	333810.259024	49.875098
3504.108614	333815.302901	49.880103
3504.007873	333819.595769	49.885108
3503.690790	333827.817877	49.890113
3504.063057	333832.468751	49.895117
3504.050134	333817.119796	49.900122
3504.032753	333821.755895	49.905127
3504.257322	333817.061659	49.910132
3504.243042	333828.341746	49.915137
3504.521476	333813.863210	49.920141
3504.108608	333823.551554	49.925146
3504.234260	333818.771124	49.930151
3504.456669	333790.885193	49.935156
3504.182863	333787.720834	49.940161
3504.377235	333785.933557	49.945165
3504.331057	333778.125354	49.950170
3504.212861	333785.552292	49.955175
3504.698586	333787.792201	49.960180
3504.520479	333775.727946	49.965185
3504.450002	333759.369766	49.970189
3504.162270	333756.513101	49.975194
3504.218130	333747.212211	49.980199
3504.437880	333749.188675	49.985204
3504.439429	333754.127280	49.990209
3504.226946	333725.469966	49.995213
3504.428535	333719.048225	50.000218
3503.916347	333716.659825	50.005223
3504.313703	333708.501462	50.010228
3504.089167	333716.378000	50.015233
3504.537855	333709.204377	50.020237
3504.199874	333707.501255	50.025242
3504.240304	333709.607899	50.030247
3504.355273	333690.139991	50.035252
3504.110622	333685.647212	50.040257
3504.086928	333674.016770	50.045261
3504.188272	333682.121831	50.050266
3504.051226	333674.633476	50.055271
3504.148605	333683.706561	50.060276
3503.910899	333685.704429	50.065281
3504.256872	333674.117379	50.070285
3503.867401	333672.931552	50.075290
3503.890900	333684.307521	50.080295
3504.403515	333672.897790	50.085300
3503.998487	333687.090948	50.090305
3503.899456	333684.382653	50.095309
3503.976708	333682.995756	50.100314
3503.826782	333673.600100	50.105319
3504.265794	333680.455263	50.110324
3504.196246	333677.182235	50.115329
3504.426939	333661.947481	50.120333
3503.928170	333663.171969	50.125338
3503.938243	333652.045342	50.130343
3503.934714	333655.228166	50.135348
3503.513345	333645.035309	50.140353
3503.738925	333655.819264	50.145357
3503.867639	333678.532792	50.150362
3503.616180	333690.028601	50.155367
3503.747073	333689.906114	50.160372
3503.809915	333691.449144	50.165377
3504.096112	333690.411082	50.170381
3504.120696	333686.283066	50.175386
3503.930436	333683.181869	50.180391
3503.823171	333682.867911	50.185396
3503.745566	333690.543021	50.190401
3504.065139	333693.751138	50.195405
3503.979316	333693.713827	50.200410
3503.946615	333683.128581	50.205415
3503.859330	333692.867304	50.210420
3503.800595	333684.551919	50.215425
3504.167590	333688.999973	50.220429
3503.862357	333703.839255	50.225434
3503.534465	333701.345346	50.230439
3503.914385	333688.098174	50.235444
3503.750164	333692.171965	50.240449
3503.922059	333705.535639	50.245453
3503.883746	333695.893221	50.250458
3504.145753	333692.440491	50.255463
3504.248921	333696.522927	50.260468
3503.735339	333706.329039	50.265473
3503.771371	333701.868263	50.270477
3503.982609	333700.358353	50.275482
3504.047308	333695.307514	50.280487
3504.154928	333702.724220	50.285492
3503.546821	333702.642186	50.290497
3503.838428	333708.527795	50.295501
3504.222311	333707.550664	50.300506
3504.187126	333700.097124	50.305511
3504.191881	333700.809228	50.310516
3504.182626	333709.517300	50.315521
3503.912892	333709.636352	50.320525
3504.294964	333715.813152	50.325530
3504.122419	333700.362117	50.330535
3504.107177	333688.526678	50.335540
3503.940708	333677.733458	50.340545
3503.962275	333669.354461	50.345549
3503.851704	333675.940097	50.350554
3504.260461	333661.848253	50.355559
3504.248840	333668.469162	50.360564
3503.940646	333675.824316	50.365569
3504.442947	333666.809250	50.370573
3504.277405	333666.580879	50.375578
3504.059163	333683.824906	50.380583
3504.297733	333682.488879	50.385588
3503.949049	333681.882135	50.390593
3503.928228	333678.499574	50.395597
3504.167197	333677.188942	50.400602
3504.273709	333676.204743	50.405607
3504.364433	333665.116284	50.410612
3504.073273	333652.331603	50.415617
3503.939101	333650.570803	50.420621
3504.196278	333655.698124	50.425626
3504.378042	333650.959728	50.430631
3504.458112	333638.370936	50.435636
3504.444706	333655.888082	50.440641
3504.303980	333651.455246	50.445645
3503.878296	333629.527007	50.450650
3504.187283	333618.531325	50.455655
3504.071402	333607.959217	50.460660
3503.801143	333609.503992	50.465665
3504.148981	333610.212776	50.470669
3504.336967	333620.620812	50.475674
3504.073399	333626.517819	50.480679
3504.171723	333623.447371	50.485684
3503.961551	333617.752619	50.490689
3504.078846	333616.181185	50.495693
3504.005836	333620.673344	50.500698
3504.049009	333610.432502	50.505703
3504.573118	333616.892351	50.510708
3504.281458	333624.397644	50.515713
3504.273102	333602.759833	50.520717
3504.171554	333593.152855	50.525722
3504.192937	333572.452274	50.530727
3504.421084	333577.456900	50.535732
3504.275388	333542.118994	50.540737
3503.719235	333509.315373	50.545741
3503.665558	333478.214354	50.550746
3503.862668	333424.390678	50.555751
3503.854534	333371.541349	50.560756
3502.735495	333308.226176	50.565761
3502.754739	333235.947994	50.570765
3502.664326	333155.285931	50.575770
3502.474191	333083.320731	50.580775
3502.001229	333007.021383	50.585780
3501.722884	332916.230988	50.590785
3501.459614	332810.163215	50.595789
3501.107226	332704.287579	50.600794
3500.250058	332600.222743	50.605799
3500.038164	332496.335787	50.610804
3499.682694	332379.385818	50.615809
3499.072486	332255.245763	50.620813
3498.627567	332128.915401	50.625818
3498.124839	331998.189649	50.630823
3497.619064	331863.263495	50.635828
3496.821215	331748.113612	50.640833
3496.901301	331607.595324	50.645837
3495.934567	331481.830039	50.650842
3495.733775	331338.453354	50.655847
3495.187938	331196.200203	50.660852
3494.426422	331060.676523	50.665857
3493.901515	330911.291059	50.670861
3493.749524	330764.544975	50.675866
3492.942834	330612.428437	50.680871
3492.585804	330466.376108	50.685876
3491.816494	330322.527226	50.690881
3491.648057	330140.852743	50.695885
3490.612238	329977.441843	50.700890
3489.553730	329832.670290	50.705895
3489.886227	329674.490672	50.710900
3488.767742	329510.353506	50.715905
3488.080517	329348.642820	50.720909
3487.729303	329191.283141	50.725914
3487.036343	329032.602355	50.730919
3486.860562	328863.961190	50.735924
3485.792008	328692.252892	50.740929
3485.305499	328516.251355	50.745933
3484.830748	328348.267352	50.750938
3484.010168	328181.381507	50.755943
3483.652430	327994.869016	50.760948
3483.048486	327828.610117	50.765953
3482.262513	327662.226882	50.770957
3481.588147	327489.282441	50.775962
3480.891618	327305.826139	50.780967
3480.238342	327134.328804	50.785972
3479.278553	326959.187837	50.790977
3478.859263	326782.178820	50.795981
3478.375220	326605.637930	50.800986
3477.220311	326440.787144	50.805991
3476.678527	326257.253034	50.810996
3475.821571	326089.502861	50.816001
3475.109079	325920.838384	50.821005
3474.761111	325748.551454	50.826010
3473.893458	325573.723882	50.831015
3473.091375	325394.048051	50.836020
3472.675536	325232.005926	50.841025
3472.446752	325075.688029	50.846029
3471.881381	324896.431977	50.851034
3470.861006	324714.294016	50.856039
3470.580650	324534.075529	50.861044
3469.387078	324357.998398	50.866049
3468.708364	324183.570843	50.871053
3468.033745	324009.244122	50.876058
3467.487203	323840.549153	50.881063
3466.800149	323661.767987	50.886068
3466.123055	323491.208837	50.891073
3465.462961	323308.756252	50.896077
3465.242196	323145.355258	50.901082
3464.218391	322967.873481	50.906087
3463.922480	322774.719334	50.911092
3462.705677	322601.188371	50.916097
3462.204001	322425.023307	50.921101
3461.599646	322252.005892	50.926106
3460.903354	322072.790035	50.931111
3460.288108	321886.049806	50.936116
3459.095578	321726.186181	50.941121
3458.640628	321548.535187	50.946125
3458.073754	321371.665386	50.951130
3457.069460	321207.544403	50.956135
3456.089289	321028.931474	50.961140
3455.764482	320860.704902	50.966145
3455.312075	320694.968005	50.971149
3454.538246	320523.068880	50.976154
3453.588633	320351.095373	50.981159
3453.365743	320187.179992	50.986164
3452.737342	320007.210859	50.991169
3451.809900	319831.897320	50.996173
3451.351977	319668.247332	51.001178
3450.572418	319496.881893	51.006183
3450.191637	319310.201113	51.011188
3449.370434	319152.820478	51.016193
3448.857657	318973.416688	51.021197
3448.176195	318797.043806	51.026202
3447.304515	318621.693709	51.031207
3446.634708	318444.681761	51.036212
3445.820611	318275.942204	51.041217
3445.242770	318086.820278	51.046221
3444.365079	317939.504331	51.051226
3443.488200	317765.146529	51.056231
3443.358583	317590.313781	51.061236
3442.547249	317419.942662	51.066241
3441.901817	317254.535750	51.071245
3441.152746	317077.381045	51.076250
3440.488833	316914.166297	51.081255
3440.365797	316743.226837	51.086260
3439.325607	316572.635801	51.091265
3438.948670	316392.161747	51.096269
3438.270570	316212.677123	51.101274
3437.469963	316035.554167	51.106279
3436.600299	315866.717391	51.111284
3435.537395	315684.619022	51.116289
3434.992554	315516.112253	51.121293
3434.375508	315351.843551	51.126298
3433.545027	315180.351244	51.131303
3433.207551	315011.912711	51.136308
3432.369649	314844.749816	51.141313
3431.604804	314680.885367	51.146317
3431.020713	314514.573035	51.151322
3430.061337	314345.085890	51.156327
3429.550484	314175.502089	51.161332
3429.052657	314014.522705	51.166337
3428.404161	313842.541077	51.171341
3427.700737	313682.001119	51.176346
3426.641145	313506.340765	51.181351
3426.197060	313346.446822	51.186356
3425.443827	313185.201007	51.191361
3424.927697	313017.347750	51.196365
3424.213991	312851.638990	51.201370
3423.654224	312686.313063	51.206375
3423.216080	312513.659456	51.211380
3422.557962	312364.492841	51.216385
3421.627761	312179.871975	51.221389
3421.121914	312022.914246	51.226394
3420.261524	311855.953975	51.231399
3419.695507	311674.941543	51.236404
3419.099729	311520.136332	51.241409
3418.536805	311344.521322	51.246413
3417.827232	311169.463981	51.251418
3417.280713	311006.781778	51.256423
3416.708736	310838.603042	51.261428
3415.541134	310683.810723	51.266433
3415.275792	310496.841113	51.271437
3414.434118	310341.258330	51.276442
3413.791559	310167.334783	51.281447
3413.357067	309985.433101	51.286452
3412.384458	309820.473868	51.291457
3411.753622	309650.214625	51.296461
3411.385948	309491.754651	51.301466
3410.371821	309321.097182	51.306471
3409.876932	309143.838365	51.311476
3409.094967	308987.251242	51.316481
3408.415037	308808.926206	51.321485
3407.591941	308642.897659	51.326490
3407.211925	308469.159327	51.331495
3406.455269	308291.253113	51.336500
3405.689040	308143.600654	51.341505
3405.083385	307965.466378	51.346509
3404.678597	307802.833816	51.351514
3403.653508	307641.317738	51.356519
3403.008570	307462.908847	51.361524
3402.505351	307297.693753	51.366529
3402.117093	307133.326086	51.371533
3401.454462	306957.185699	51.376538
3400.356336	306796.826045	51.381543
3399.975340	306620.207755	51.386548
3399.272577	306460.192616	51.391553
3398.465378	306277.733290	51.396557
3397.724184	306121.187116	51.401562
3397.079652	305937.810309	51.406567
3396.903794	305773.993062	51.411572
3395.759549	305616.211290	51.416577
3395.118261	305438.639438	51.421581
3394.636563	305279.275501	51.426586
3393.609291	305107.977866	51.431591
3392.882205	304922.550026	51.436596
3392.431022	304776.142715	51.441601
3391.635143	304598.008513	51.446605
3390.845777	304434.566807	51.451610
3390.377258	304280.445590	51.456615
3389.628568	304106.377833	51.461620
3388.843938	303954.037926	51.466625
3388.416527	303784.859350	51.471629
3387.524616	303625.736667	51.476634
3386.896729	303456.258351	51.481639
3386.423402	303280.490766	51.486644
3385.519834	303126.462578	51.491649
3384.809133	302962.242784	51.496653
3383.856909	302790.675844	51.501658
3383.346658	302638.138382	51.506663
3382.986797	302480.585625	51.511668
3382.317934	302317.835543	51.516673
3381.923318	302163.216559	51.521677
3381.146649	301995.746474	51.526682
3379.951261	301823.147312	51.531687
3379.761446	301668.571843	51.536692
3378.833128	301492.950530	51.541697
3378.383770	301330.648555	51.546701
3377.696964	301168.689559	51.551706
3377.081627	301006.719095	51.556711
3376.336106	300850.015130	51.561716
3375.672397	300681.405262	51.566721
3375.133972	300508.038649	51.571725
3374.211020	300344.486316	51.576730
3373.455267	300189.464118	51.581735
3373.144372	300018.200191	51.586740
3372.150463	299860.210298	51.591745
3371.759955	299699.425379	51.596749
3371.169062	299540.123592	51.601754
3369.972748	299380.408064	51.606759
3369.620263	299209.862957	51.611764
3368.820492	299051.714278	51.616769
3368.034264	298898.860382	51.621773
3367.720738	298732.867179	51.626778
3366.891771	298567.362800	51.631783
3366.062530	298390.321872	51.636788
3365.536220	298252.171559	51.641793
3365.237285	298087.372383	51.646797
3364.589138	297917.942388	51.651802
3363.595492	297759.033745	51.656807
3363.285394	297587.869171	51.661812
3362.201244	297435.188476	51.666817
3361.505036	297266.223885	51.671821
3361.040057	297103.156368	51.676826
3360.400947	296943.987226	51.681831
3359.559051	296776.751522	51.686836
3358.690179	296626.480957	51.691841
3358.101472	296453.271121	51.696845
3357.230656	296306.591465	51.701850
3356.757897	296137.717876	51.706855
3356.372359	295989.000275	51.711860
3355.589232	295817.730657	51.716865
3354.557976	295663.053763	51.721869
3354.228414	295503.172350	51.726874
3353.319433	295348.908820	51.731879
3352.954745	295189.389258	51.736884
3352.467798	295035.746363	51.741889
3351.890724	294866.990083	51.746893
3351.122309	294705.573024	51.751898
3350.438644	294541.621181	51.756903
3350.053074	294382.919262	51.761908
3348.934198	294226.396050	51.766913
3348.160145	294052.780559	51.771917
3347.506658	293890.962706	51.776922
3347.128300	293735.824604	51.781927
3346.176176	293579.045354	51.786932
3345.470031	293410.181020	51.791937
3344.965529	293253.610894	51.796941
3344.264192	293089.431565	51.801946
3343.511483	292942.679973	51.806951
3343.193513	292769.067770	51.811956
3342.455897	292605.123045	51.816961
3341.561925	292457.833208	51.821965
3340.672043	292302.469435	51.826970
3340.216040	292142.299983	51.831975
3339.620580	291972.551219	51.836980
3338.921820	291818.990575	51.841985
3338.440541	291651.821225	51.846989
3337.723772	291499.129131	51.851994
3336.657928	291329.759936	51.856999
3336.363042	291169.029562	51.862004
3335.602965	291021.564897	51.867009
3335.029375	290856.472508	51.872013
3334.155045	290705.307458	51.877018
3333.366384	290547.685451	51.882023
3332.928063	290384.685195	51.887028
3332.069032	290238.050716	51.892033
3331.553847	290074.476675	51.897037
3330.947827	289920.798388	51.902042
3329.959974	289762.978228	51.907047
3329.741226	289598.924076	51.912052
3328.715844	289450.787432	51.917057
3328.107033	289281.854043	51.922061
3327.586077	289134.605237	51.927066
3326.689474	288972.593498	51.932071
3325.920436	288814.891028	51.937076
3325.577641	288664.506739	51.942081
3324.755827	288509.384712	51.947085
3324.168176	288352.468290	51.952090
3323.391834	288209.003210	51.957095
3322.919381	288046.185336	51.962100
3322.243656	287891.854877	51.967105
3321.314417	287738.455818	51.972109
3321.059937	287581.384457	51.977114
3320.191470	287420.233389	51.982119
3319.474706	287264.559330	51.987124
3318.741354	287112.631616	51.992129
3318.070621	286947.628858	51.997133
3317.667111	286796.158199	52.002138
3316.571932	286647.598353	52.007143
3316.435998	286483.325774	52.012148
3315.706437	286335.752163	52.017153
3314.918448	286174.154849	52.022157
3314.727870	286024.101874	52.027162
3313.471777	285865.838377	52.032167
3313.079045	285699.950653	52.037172
3312.274984	285548.262699	52.042177
3311.508534	285384.267654	52.047181
3311.214257	285225.877248	52.052186
3310.224494	285063.649228	52.057191
3309.925533	284920.540311	52.062196
3309.041464	284757.989840	52.067201
3308.412857	284600.339722	52.072205
3307.744709	284444.096550	52.077210
3306.795761	284293.679007	52.082215
3306.108449	284127.480712	52.087220
3305.833947	283980.674745	52.092225
3305.058869	283821.010075	52.097229
3304.518061	283656.189194	52.102234
3303.673572	283499.158621	52.107239
3302.802356	283349.288791	52.112244
3302.296183	283183.596360	52.117249
3301.495974	283026.813323	52.122253
3301.161153	282876.425558	52.127258
3300.653695	282720.869540	52.132263
3300.117686	282563.280536	52.137268
3299.135010	282396.746380	52.142273
3298.571312	282240.231334	52.147277
3298.045352	282075.611373	52.152282
3296.968927	281915.891937	52.157287
3296.676244	281769.623083	52.162292
3295.856338	281598.707893	52.167297
3295.049873	281448.954675	52.172301
3294.378674	281281.097545	52.177306
3293.530072	281130.408596	52.182311
3293.271897	280977.792509	52.187316
3292.283391	280816.403471	52.192321
3291.756523	280669.560190	52.197325
3291.167231	280488.344531	52.202330
3290.428959	280347.290468	52.207335
3289.847512	280176.846599	52.212340
3289.135529	280028.682662	52.217345
3288.452746	279862.075010	52.222349
3287.742364	279712.127985	52.227354
3287.047797	279566.533522	52.232359
3286.810482	279399.320492	52.237364
3285.820072	279250.334552	52.242369
3284.972812	279087.012736	52.247373
3284.184294	278930.940085	52.252378
3283.353512	278779.152783	52.257383
3283.188280	278627.285657	52.262388
3282.238464	278470.932841	52.267393
3281.768874	278311.600653	52.272397
3281.288502	278144.706047	52.277402
3280.385817	278005.027508	52.282407
3279.446680	277836.932016	52.287412
3278.952429	277687.307116	52.292417
3278.332816	277535.155196	52.297421
3277.794129	277385.562769	52.302426
3276.975620	277235.377884	52.307431
3276.422383	277082.680596	52.312436
3275.687999	276930.215699	52.317441
3275.118401	276766.467701	52.322445
3274.229531	276620.394321	52.327450
3273.357881	276468.995319	52.332455
3272.945412	276313.117646	52.337460
3272.119568	276166.550382	52.342465
3271.369945	276006.396404	52.347469
3270.879680	275863.367094	52.352474
3270.022945	275727.144876	52.357479
3269.390751	275559.535545	52.362484
3268.970182	275413.439000	52.367489
3268.303334	275252.431465	52.372493
3267.836615	275113.371497	52.377498
3266.747236	274956.709493	52.382503
3266.449735	274811.586753	52.387508
3265.481405	274647.010406	52.392513
3264.810833	274497.336909	52.397517
3264.332101	274358.890100	52.402522
3263.500208	274205.854837	52.407527
3263.156028	274049.711695	52.412532
3262.145608	273902.409607	52.417537
3261.722860	273753.995830	52.422541
3261.057864	273603.455570	52.427546
3259.771338	273451.893030	52.432551
3259.368514	273302.864891	52.437556
3259.001093	273158.058914	52.442561
3257.979375	273017.864352	52.447565
3257.582935	272858.546017	52.452570
3256.832944	272718.588650	52.457575
3256.560153	272564.369929	52.462580
3255.847200	272411.698017	52.467585
3255.332560	272248.476319	52.472589
3254.557918	272099.354305	52.477594
3253.460621	271942.922994	52.482599
3253.114285	271798.903341	52.487604
3252.426151	271643.247803	52.492609
3251.670419	271484.368501	52.497613
3251.086950	271340.564700	52.502618
3250.558342	271192.881053	52.507623
3249.713833	271035.212879	52.512628
3248.882537	270882.687244	52.517633
3248.441461	270734.454990	52.522637
3248.011285	270569.080857	52.527642
3247.183256	270434.891975	52.532647
3246.733948	270270.845281	52.537652
3245.942635	270112.481219	52.542657
3244.663266	269964.152502	52.547661
3244.188298	269814.474086	52.552666
3243.522093	269675.981065	52.557671
3243.057479	269517.539982	52.562676
3242.183074	269371.923369	52.567681
3241.361762	269233.276696	52.572685
3240.978183	269072.174199	52.577690
3240.107273	268939.520478	52.582695
3239.436972	268780.857429	52.587700
3238.732770	268640.868010	52.592705
3238.156351	268505.977527	52.597709
3237.725505	268342.310407	52.602714
3236.834489	268210.602353	52.607719
3236.576146	268054.701304	52.612724
3235.851808	267912.550450	52.617729
3234.741577	267752.709338	52.622733
3234.671102	267593.238622	52.627738
3233.471570	267461.197534	52.632743
3233.135286	267303.933754	52.637748
3232.432514	267156.176694	52.642753
3231.686115	267004.733696	52.647757
3230.783758	266854.436016	52.652762
3230.116918	266717.650185	52.657767
3230.022806	266574.508625	52.662772
3229.399948	266419.506199	52.667777
3228.560705	266261.634690	52.672781
3227.821753	266115.921134	52.677786
3226.925364	265962.286482	52.682791
3226.404683	265817.226136	52.687796
3225.854276	265673.825968	52.692801
3225.188509	265519.110801	52.697805
3224.513359	265359.125284	52.702810
3223.762497	265219.551730	52.707815
3222.988319	265067.528034	52.712820
3222.074440	264925.357163	52.717825
3221.600194	264768.447204	52.722829
3221.165676	264627.423075	52.727834
3220.191170	264483.453731	52.732839
3219.994562	264329.021365	52.737844
3218.999486	264188.569976	52.742849
3218.463480	264040.380150	52.747853
3217.851921	263881.556724	52.752858
3216.935444	263747.154453	52.757863
3216.342018	263590.416663	52.762868
3215.488084	263461.862238	52.767873
3215.032377	263314.627799	52.772877
3214.735538	263156.162405	52.777882
3213.708170	263015.665665	52.782887
3213.235639	262860.615440	52.787892
3212.588993	262716.645898	52.792897
3212.176706	262563.369038	52.797901
3211.114431	262415.441463	52.802906
3210.453742	262266.992003	52.807911
3210.027025	262105.415130	52.812916
3208.852236	261970.825249	52.817921
3208.222869	261825.860141	52.822925
3207.959386	261666.549780	52.827930
3206.906056	261537.187246	52.832935
3206.251827	261385.273581	52.837940
3205.886409	261233.314302	52.842945
3204.930993	261093.927645	52.847949
3204.439197	260948.635595	52.852954
3203.249781	260801.085491	52.857959
3203.181702	260657.534765	52.862964
3202.443138	260520.278842	52.867969
3201.957996	260372.464739	52.872973
3201.332919	260219.171839	52.877978
3200.347075	260080.681877	52.882983
3199.965654	259933.513766	52.887988
3199.310057	259783.103790	52.892993
3198.551764	259634.289140	52.897997
3198.132077	259491.049345	52.903002
3196.807110	259347.188829	52.908007
3196.652923	259185.137590	52.913012
3195.975091	259050.215847	52.918017
3195.332006	258902.885986	52.923021
3194.572794	258749.844393	52.928026
3193.760797	258596.327364	52.933031
3193.108032	258454.882300	52.938036
3192.339337	258304.287368	52.943041
3192.243519	258165.071899	52.948045
3191.242481	258012.629320	52.953050
3190.239579	257877.479522	52.958055
3189.781028	257729.688242	52.963060
3188.876372	257588.385422	52.968065
3188.058451	257441.389740	52.973069
3187.452579	257304.369280	52.978074
3186.787640	257156.279950	52.983079
3186.399458	257029.488560	52.988084
3185.399227	256883.438913	52.993089
3184.802466	256740.177865	52.998093
3184.338229	256592.235431	53.003098
3183.483792	256465.416267	53.008103
3183.230376	256314.843006	53.013108
3182.510412	256169.080573	53.018113
3181.806743	256035.718198	53.023117
3181.102768	255880.199490	53.028122
3180.551599	255754.631597	53.033127
3179.751281	255603.050287	53.038132
3179.183505	255456.143718	53.043137
3178.339174	255314.068832	53.048141
3178.088782	255164.591011	53.053146
3176.805250	255032.441586	53.058151
3176.573165	254877.230987	53.063156
3176.016940	254739.873267	53.068161
3174.904874	254596.848037	53.073165
3174.462243	254442.002165	53.078170
3173.773299	254311.541840	53.083175
3173.264519	254167.682931	53.088180
3172.463342	254033.191303	53.093185
3171.553794	253879.387504	53.098189
3171.099199	253716.292820	53.103194
3170.475943	253600.720740	53.108199
3169.754156	253455.953799	53.113204
3169.181006	253318.523378	53.118209
3168.556459	253168.469635	53.123213
3168.057455	253021.146568	53.128218
3166.992415	252876.739997	53.133223
3166.740196	252742.646316	53.138228
3166.050603	252598.155096	53.143233
3165.169892	252452.268095	53.148237
3164.743070	252300.553918	53.153242
3163.307829	252170.977194	53.158247
3163.032107	252031.030427	53.163252
3162.503221	251882.516096	53.168257
3161.727794	251744.940625	53.173261
3161.197173	251605.976799	53.178266
3160.354821	251456.697502	53.183271
3159.928156	251319.856655	53.188276
3159.152535	251171.916779	53.193281
3158.464691	251047.468759	53.198285
3158.157023	250900.015344	53.203290
3157.014565	250767.464714	53.208295
3156.511424	250618.947419	53.213300
3156.109330	250476.322487	53.218305
3155.336077	250327.975527	53.223309
3154.689798	250190.228103	53.228314
3153.802874	250043.198177	53.233319
3153.034127	249899.358448	53.238324
3152.405264	249761.634103	53.243329
3151.636745	249619.348038	53.248333
3151.204564	249481.490950	53.253338
3150.632044	249350.786745	53.258343
3149.646506	249204.919183	53.263348
3149.018975	249074.631375	53.268353
3148.335618	248932.790851	53.273357
3148.149603	248783.919497	53.278362
3147.376383	248649.427715	53.283367
3146.755193	248502.637319	53.288372
3145.784598	248366.852780	53.293377
3145.036294	248228.562979	53.298381
3144.483777	248082.678906	53.303386
3143.613427	247955.893863	53.308391
3142.956242	247812.776949	53.313396
3142.336853	247671.462278	53.318401
3141.616977	247538.516481	53.323405
3140.971669	247398.785064	53.328410
3140.360958	247268.216038	53.333415
3139.944911	247128.601400	53.338420
3139.051028	246987.254431	53.343425
3138.357340	246861.155432	53.348429
3138.082107	246702.979790	53.353434
3137.278374	246580.259941	53.358439
3136.629788	246434.851109	53.363444
3135.827551	246286.003400	53.368449
3135.332118	246156.741372	53.373453
3134.460081	246015.646576	53.378458
3133.721688	245873.130164	53.383463
3133.299946	245748.466143	53.388468
3132.784463	245604.361332	53.393473
3131.984697	245466.260607	53.398477
3131.267841	245326.950020	53.403482
3130.525778	245175.572900	53.408487
3129.835389	245042.039097	53.413492
3129.209490	244898.130768	53.418497
3128.644432	244774.508940	53.423501
3128.073453	244620.278709	53.428506
3127.330237	244493.298432	53.433511
3126.785079	244342.680527	53.438516
3125.927592	244212.306243	53.443521
3124.969819	244072.423925	53.448525
3124.609623	243935.604895	53.453530
3123.819242	243802.215498	53.458535
3122.987753	243652.585917	53.463540
3122.385978	243521.815352	53.468545
3121.680416	243398.777297	53.473549
3121.167968	243266.490412	53.478554
3120.379218	243140.715533	53.483559
3119.841540	242992.007911	53.488564
3119.434888	242856.496109	53.493569
3118.563258	242729.410573	53.498573
3117.864688	242585.134349	53.503578
3117.060951	242441.893535	53.508583
3116.318245	242311.732226	53.513588
3115.621684	242180.137715	53.518593
3114.897774	242033.446977	53.523597
3114.504964	241898.978095	53.528602
3113.540205	241783.010966	53.533607
3113.179138	241645.685277	53.538612
3112.486730	241517.248466	53.543617
3111.444338	241388.892640	53.548621
3111.334067	241243.480853	53.553626
3110.344312	241120.821090	53.558631
3109.695683	240981.988319	53.563636
3109.093459	240851.373455	53.568641
3108.686902	240705.729101	53.573645
3108.152573	240578.414197	53.578650
3107.113821	240451.510296	53.583655
3106.670815	240300.168149	53.588660
3106.192495	240166.529625	53.593665
3105.372889	240039.285921	53.598669
3104.662472	239894.862034	53.603674
3103.686336	239764.842315	53.608679
3103.084276	239626.487617	53.613684
3102.300215	239499.442604	53.618689
3101.915882	239356.597515	53.623693
3101.373252	239224.319879	53.628698
3100.253088	239099.620291	53.633703
3099.814687	238963.328577	53.638708
3099.274135	238831.687681	53.643713
3098.346814	238700.006291	53.648717
3097.969218	238569.587663	53.653722
3097.079665	238438.486283	53.658727
3096.582423	238286.467881	53.663732
3095.781377	238166.378772	53.668737
3095.283155	238039.723078	53.673741
3094.638501	237888.085055	53.678746
3093.684451	237763.666259	53.683751
3093.215473	237629.774648	53.688756
3092.629508	237504.177487	53.693761
3091.828739	237376.169934	53.698765
3091.482601	237231.411767	53.703770
3090.819390	237099.130315	53.708775
3090.477401	236969.446425	53.713780
3089.155133	236831.412936	53.718785
3088.423987	236690.281361	53.723789
3087.969788	236558.527709	53.728794
3086.950923	236419.962935	53.733799
3086.354758	236292.280805	53.738804
3085.864493	236163.054257	53.743809
3085.020126	236030.828283	53.748813
3084.813486	235890.174982	53.753818
3083.957395	235758.766043	53.758823
3083.326219	235629.511536	53.763828
3082.964645	235504.415990	53.768833
3081.992220	235362.127627	53.773837
3081.656835	235233.157834	53.778842
3080.795618	235100.757484	53.783847
3080.016047	234967.758730	53.788852
3079.278783	234825.306589	53.793857
3078.656298	234702.392239	53.798861
3077.948228	234570.986878	53.803866
3076.944420	234437.998852	53.808871
3076.487723	234297.540114	53.813876
3075.976278	234171.578734	53.818881
3075.028640	234045.202748	53.823885
3074.929745	233901.479602	53.828890
3074.208129	233783.725608	53.833895
3073.760691	233638.046432	53.838900
3073.081875	233507.579987	53.843905
3072.467703	233376.517841	53.848909
3071.967918	233227.893869	53.853914
3070.736256	233090.411348	53.858919
3070.476541	232954.863149	53.863924
3069.619447	232816.965260	53.868929
3068.747849	232696.028024	53.873933
3068.632886	232540.240120	53.878938
3067.394871	232414.319625	53.883943
3066.732498	232284.743432	53.888948
3066.175068	232147.512042	53.893953
3065.204253	232010.524513	53.898957
3064.948321	231878.058215	53.903962
3064.360628	231749.642214	53.908967
3063.525361	231610.138500	53.913972
3062.943579	231485.337590	53.918977
3062.070853	231351.110904	53.923981
3061.807148	231213.477928	53.928986
3060.977746	231078.302677	53.933991
3060.080114	230936.620095	53.938996
3059.364025	230803.718915	53.944001
3058.723350	230672.104563	53.949005
3058.259385	230551.563915	53.954010
3057.520006	230417.546652	53.959015
3057.098017	230283.021038	53.964020
3056.155593	230143.943908	53.969025
3055.225581	230019.352886	53.974029
3054.857051	229890.497416	53.979034
3054.218427	229756.439729	53.984039
3053.625915	229625.990528	53.989044
3053.309089	229485.364083	53.994049
3052.016005	229349.551878	53.999053
3051.694461	229214.197198	54.004058
3050.534274	229085.519113	54.009063
3050.114815	228949.085484	54.014068
3049.407344	228808.241868	54.019073
3048.763381	228690.482079	54.024077
3047.896257	228543.527917	54.029082
3047.423658	228427.345440	54.034087
3046.606691	228293.572824	54.039092
3046.003276	228170.282185	54.044097
3045.230820	228045.057950	54.049101
3044.631479	227915.605375	54.054106
3043.713858	227784.930304	54.059111
3043.489407	227656.335392	54.064116
3042.768939	227530.849067	54.069121
3041.970880	227408.659704	54.074125
3041.649528	227271.805819	54.079130
3040.699283	227143.504785	54.084135
3039.985290	227017.025213	54.089140
3039.417159	226883.648262	54.094145
3038.801412	226743.939269	54.099149
3038.155541	226623.509227	54.104154
3037.040621	226501.778707	54.109159
3036.899862	226368.831423	54.114164
3036.298535	226243.710076	54.119169
3035.544193	226109.969191	54.124173
3035.080750	225977.480980	54.129178
3034.008494	225858.328922	54.134183
3033.188192	225729.118376	54.139188
3033.047804	225592.480480	54.144193
3032.156532	225456.547255	54.149197
3031.400796	225323.075210	54.154202
3030.638107	225212.073400	54.159207
3029.920380	225075.018541	54.164212
3029.652076	224946.994890	54.169217
3028.882523	224820.043735	54.174221
3028.378993	224683.668529	54.179226
3027.489133	224555.692959	54.184231
3026.865282	224420.826673	54.189236
3026.015992	224302.965548	54.194241
3025.512732	224171.224937	54.199245
3024.720115	224047.868547	54.204250
3023.695202	223922.410466	54.209255
3023.517412	223790.988142	54.214260
3022.574967	223656.733703	54.219265
3021.690268	223541.718110	54.224269
3021.203723	223416.697551	54.229274
3020.418517	223291.571705	54.234279
3019.998059	223171.263892	54.239284
3019.193235	223062.690440	54.244289
3018.649485	222922.034655	54.249293
3018.186524	222793.943455	54.254298
3017.069524	222680.658976	54.259303
3016.473469	222565.280892	54.264308
3016.226761	222439.116446	54.269313
3015.365052	222306.913789	54.274317
3015.285345	222187.610143	54.279322
3014.395972	222050.880506	54.284327
3013.840191	221931.627154	54.289332
3012.652387	221788.834952	54.294337
3012.199767	221675.243125	54.299341
3011.940009	221548.152947	54.304346
3010.798695	221422.831916	54.309351
3010.230694	221287.593073	54.314356
3010.018135	221156.791762	54.319361
3009.262299	221027.451467	54.324365
3008.303564	220894.821096	54.329370
3007.723011	220779.876077	54.334375
3007.240762	220639.647579	54.339380
3006.646345	220516.214574	54.344385
3005.492420	220386.849297	54.349389
3005.207185	220243.777148	54.354394
3004.358345	220125.464117	54.359399
3003.630768	219996.044768	54.364404
3003.162870	219872.389142	54.369409
3002.182863	219735.028886	54.374413
3001.622711	219606.793011	54.379418
3000.724842	219489.367093	54.384423
3000.271454	219353.158941	54.389428
2999.664104	219230.544818	54.394433
2998.577902	219105.371747	54.399437
2998.440481	218964.328111	54.404442
2997.531655	218849.730852	54.409447
2996.877291	218731.211094	54.414452
2996.396250	218602.404390	54.419457
2995.553724	218483.405660	54.424461
2994.781596	218351.272262	54.429466
2994.248288	218238.907779	54.434471
2993.891313	218099.135319	54.439476
2992.700802	217973.917091	54.444481
2992.129139	217856.289457	54.449485
2991.635736	217736.829382	54.454490
2990.635987	217606.299070	54.459495
2990.200039	217484.526382	54.464500
2989.941152	217361.223861	54.469505
2988.914630	217227.974496	54.474509
2988.417853	217102.978954	54.479514
2987.707584	216980.117693	54.484519
2987.303101	216857.131872	54.489524
2986.428868	216724.763110	54.494529
2985.846965	216597.592591	54.499533
2985.310581	216461.708617	54.504538
2984.161580	216341.501879	54.509543
2983.503031	216218.137361	54.514548
2983.061986	216100.364722	54.519553
2982.626715	215970.079073	54.524557
2981.721751	215847.925265	54.529562
2980.869695	215719.042579	54.534567
2980.114016	215592.881533	54.539572
2979.564900	215465.033304	54.544577
2978.616560	215369.095396	54.549581
2978.378503	215236.870642	54.554586
2977.745909	215112.511186	54.559591
2976.953301	214991.499429	54.564596
2976.548266	214858.741793	54.569601
2975.584260	214750.804290	54.574605
2975.113886	214598.442962	54.579610
2974.455698	214499.711021	54.584615
2973.757172	214359.185590	54.589620
2973.385516	214243.645391	54.594625
2972.353754	214119.172769	54.599629
2971.936105	213988.608130	54.604634
2971.027213	213856.835956	54.609639
2970.415650	213735.186857	54.614644
2969.667665	213614.412371	54.619649
2968.862857	213488.746738	54.624653
2968.569784	213371.515497	54.629658
2967.336062	213246.872840	54.634663
2967.010632	213114.666127	54.639668
2966.768668	212988.403226	54.644673
2966.063091	212884.984526	54.649677
2965.451520	212755.229448	54.654682
2964.931009	212617.403360	54.659687
2963.946002	212490.597194	54.664692
2963.178580	212361.682168	54.669697
2962.543975	212243.005119	54.674701
2961.839924	212109.702143	54.679706
2960.977616	211987.154133	54.684711
2960.252229	211861.720904	54.689716
2959.652630	211740.226377	54.694721
2958.883642	211631.295828	54.699725
2958.299380	211502.888100	54.704730
2957.508464	211387.037503	54.709735
2957.020354	211262.293374	54.714740
2956.519511	211144.297215	54.719745
2955.803106	211022.237072	54.724749
2954.998417	210893.394547	54.729754
2954.581030	210776.964096	54.734759
2953.871317	210653.567200	54.739764
2953.247734	210531.442402	54.744769
2952.265658	210409.120041	54.749773
2951.933882	210289.736863	54.754778
2951.242312	210159.579721	54.759783
2950.685554	210032.850669	54.764788
2949.837658	209906.155237	54.769793
2948.819040	209790.929095	54.774797
2948.394723	209669.347173	54.779802
2947.558553	209550.007082	54.784807
2946.980975	209431.008105	54.789812
2946.296317	209299.833479	54.794817
2945.721421	209192.467363	54.799821
2945.302667	209070.631192	54.804826
2944.745319	208958.642686	54.809831
2943.879946	208828.375860	54.814836
2943.171330	208708.431754	54.819841
2942.579486	208582.220327	54.824845
2942.077699	208450.064026	54.829850
2940.994729	208335.818070	54.834855
2940.371287	208217.974158	54.839860
2940.081854	208096.603090	54.844865
2939.086312	207986.060274	54.849869
2938.488405	207854.009580	54.854874
2937.950005	207744.731178	54.859879
2937.528082	207613.938581	54.864884
2936.728474	207487.622331	54.869889
2935.825209	207365.917196	54.874893
2935.322632	207236.258166	54.879898
2934.537076	207125.060071	54.884903
2933.734428	207011.535868	54.889908
2933.458102	206869.076738	54.894913
2932.571732	206760.707923	54.899917
2931.904043	206622.142125	54.904922
2931.164539	206508.328898	54.909927
2930.787526	206384.811612	54.914932
2930.258878	206273.358086	54.919937
2928.940636	206154.393750	54.924941
2928.616164	206023.423776	54.929946
2927.688985	205908.559652	54.934951
2927.171922	205791.492749	54.939956
2926.702813	205666.387998	54.944961
2925.741085	205547.432086	54.949965
2925.040408	205434.442022	54.954970
2924.715420	205313.056819	54.959975
2923.997260	205183.907317	54.964980
2923.841220	205070.017238	54.969985
2922.962633	204946.824202	54.974989
2922.235526	204815.564347	54.979994
2921.176152	204697.821923	54.984999
2920.496786	204573.910917	54.990004
2920.116756	204458.784869	54.995009
2919.211577	204337.659016	55.000013
2918.467031	204201.490966	55.005018
2917.992755	204090.542075	55.010023
2917.037272	203974.146399	55.015028
2916.599172	203853.558481	55.020033
2915.677672	203744.653633	55.025037
2915.527056	203620.686432	55.030042
2914.425083	203511.746973	55.035047
2913.878792	203388.873741	55.040052
2913.668578	203270.528955	55.045057
2912.627732	203149.287126	55.050061
2912.173532	203028.029034	55.055066
2911.384136	202917.857713	55.060071
2910.785062	202789.674677	55.065076
2910.408069	202656.824530	55.070081
2909.188501	202553.008648	55.075085
2908.729253	202418.721336	55.080090
2907.800817	202312.887295	55.085095
2907.226504	202192.375404	55.090100
2906.621663	202072.963026	55.095105
2906.026749	201952.938495	55.100109
2905.587520	201827.226616	55.105114
2904.568053	201717.603125	55.110119
2904.008604	201595.919410	55.115124
2903.445652	201485.193319	55.120129
2902.771259	201365.818932	55.125133
2902.009590	201241.953754	55.130138
2901.619872	201119.022559	55.135143
2900.495100	200993.382949	55.140148
2900.000756	200881.590991	55.145153
2899.451773	200764.781339	55.150157
2898.538747	200647.622362	55.155162
2897.941275	200539.690528	55.160167
2897.569644	200421.364654	55.165172
2897.074429	200295.232487	55.170177
2895.941761	200182.245043	55.175181
2895.216473	200052.243182	55.180186
2894.852320	199940.788856	55.185191
2893.946649	199829.471401	55.190196
2893.364354	199707.986396	55.195201
2892.609369	199596.034753	55.200205
2892.205414	199469.012026	55.205210
2891.569196	199357.118429	55.210215
2890.711601	199225.676119	55.215220
2890.207414	199110.046392	55.220225
2889.436575	199002.704993	55.225229
2888.660225	198886.787991	55.230234
2888.021174	198762.909081	55.235239
2887.171984	198642.601284	55.240244
2886.813304	198531.047227	55.245249
2885.957836	198417.128874	55.250253
2885.215375	198296.932213	55.255258
2884.549457	198194.347683	55.260263
2883.880792	198068.337306	55.265268
2883.334068	197960.135419	55.270273
2882.148716	197851.907626	55.275277
2881.971824	197732.093521	55.280282
2881.416764	197629.009000	55.285287
2880.217865	197508.097480	55.290292
2879.907528	197394.820338	55.295297
2879.265749	197297.094578	55.300301
2878.892912	197161.877773	55.305306
2878.245736	197051.645003	55.310311
2877.307744	196938.061049	55.315316
2877.173974	196813.126941	55.320321
2876.168082	196706.489131	55.325325
2875.417644	196585.928658	55.330330
2874.709502	196479.676805	55.335335
2873.900414	196356.441290	55.340340
2873.548293	196240.030347	55.345345
2873.178601	196125.162101	55.350349
2872.416980	196009.032837	55.355354
2871.547353	195889.129087	55.360359
2870.967748	195771.889972	55.365364
2870.396890	195650.807010	55.370369
2869.460201	195540.356109	55.375373
2869.012680	195424.916443	55.380378
2868.122469	195303.630389	55.385383
2867.719413	195193.566538	55.390388
2867.088604	195078.691095	55.395393
2866.147566	194955.428958	55.400397
2865.633673	194832.722964	55.405402
2864.903452	194721.134160	55.410407
2864.163247	194603.986791	55.415412
2863.725497	194485.061341	55.420417
2862.880280	194371.532028	55.425421
2862.006074	194258.669207	55.430426
2861.662278	194136.599619	55.435431
2860.988384	194029.367727	55.440436
2860.332478	193902.411272	55.445441
2859.252074	193801.657051	55.450445
2858.869327	193675.917575	55.455450
2857.789678	193565.888081	55.460455
2857.044179	193453.693781	55.465460
2857.070045	193333.348943	55.470465
2856.051445	193226.147918	55.475469
2855.648727	193109.993953	55.480474
2855.080597	192999.312155	55.485479
2853.958386	192882.343833	55.490484
2853.397401	192762.729488	55.495489
2852.695493	192662.273911	55.500493
2852.193817	192539.329879	55.505498
2851.426150	192439.457727	55.510503
2850.822744	192319.558538	55.515508
2850.311490	192210.510830	55.520513
2849.343661	192094.181558	55.525517
2848.763641	191980.870200	55.530522
2848.308630	191868.124583	55.535527
2847.781204	191754.131088	55.540532
2847.220003	191639.278028	55.545537
2846.500417	191533.687377	55.550541
2845.925317	191399.777703	55.555546
2845.064588	191289.247893	55.560551
2844.090446	191183.800101	55.565556
2843.952721	191055.534805	55.570561
2842.977162	190948.484641	55.575565
2842.135231	190834.581283	55.580570
2841.533330	190728.146760	55.585575
2841.066827	190597.122962	55.590580
2840.392730	190496.642014	55.595585
2839.418182	190379.325542	55.600589
2838.895405	190263.362780	55.605594
2838.139059	190159.002363	55.610599
2837.415769	190054.089858	55.615604
2837.230594	189928.150642	55.620609
2836.657471	189823.914618	55.625613
2835.886962	189713.450491	55.630618
2835.351965	189588.445440	55.635623
2834.277949	189477.711857	55.640628
2833.616550	189359.928460	55.645633
2832.104113	189252.127430	55.650637
2831.736081	189147.491460	55.655642
2831.533514	189031.620945	55.660647
2830.619326	188937.046416	55.665652
2830.151793	188815.175192	55.670657
2829.456935	188723.047248	55.675661
2828.660989	188618.594720	55.680666
2828.287870	188494.101277	55.685671
2827.394084	188395.606106	55.690676
2826.886396	188283.818751	55.695681
2826.148083	188177.322505	55.700685
2825.696879	188059.572694	55.705690
2825.001385	187957.790140	55.710695
2824.220436	187836.301878	55.715700
2823.543252	187733.117471	55.720705
2822.874400	187626.089877	55.725709
2822.294033	187513.501662	55.730714
2821.714549	187408.356018	55.735719
2820.942250	187286.956881	55.740724
2820.410614	187181.409791	55.745729
2819.547003	187085.546088	55.750733
2818.884258	186961.776883	55.755738
2818.462968	186854.533765	55.760743
2817.745836	186747.363191	55.765748
2816.905965	186631.854016	55.770753
2816.179827	186530.193959	55.775757
2815.323985	186424.483679	55.780762
2814.860822	186313.635454	55.785767
2814.337175	186206.053852	55.790772
2813.635193	186095.396639	55.795777
2812.905706	185989.438365	55.800781
2812.589116	185886.557207	55.805786
2811.685291	185776.492489	55.810791
2810.466574	185662.801356	55.815796
2810.001304	185559.562836	55.820801
2809.695615	185447.699497	55.825805
2808.859877	185337.294303	55.830810
2808.474081	185229.604133	55.835815
2807.758012	185134.700726	55.840820
2807.277762	185014.062841	55.845825
2806.318084	184914.097179	55.850829
2805.695989	184798.418247	55.855834
2805.017483	184689.872506	55.860839
2804.553973	184579.613764	55.865844
2804.108675	184459.938652	55.870849
2803.563162	184351.716143	55.875853
2802.718706	184235.781290	55.880858
2801.876860	184130.315869	55.885863
2801.063967	184024.235497	55.890868
2800.797237	183907.281358	55.895873
2799.814897	183788.456368	55.900877
2799.163383	183687.948525	55.905882
2798.550453	183556.560840	55.910887
2797.772506	183466.504771	55.915892
2796.937692	183351.690148	55.920897
2796.295071	183250.265980	55.925901
2795.934196	183133.710421	55.930906
2795.274936	183033.688686	55.935911
2794.481432	182910.205749	55.940916
2794.118005	182805.672664	55.945921
2793.228116	182694.125006	55.950925
2792.795932	182592.249241	55.955930
2792.165362	182469.466822	55.960935
2791.518178	182362.461030	55.965940
2790.800965	182234.973617	55.970945
2789.812955	182133.632171	55.975949
2789.266813	182016.434728	55.980954
2788.590863	181911.050114	55.985959
2787.535878	181807.811951	55.990964
2786.930966	181702.594678	55.995969
2786.324374	181601.181346	56.000973
2785.947629	181490.547695	56.005978
2785.397134	181378.720685	56.010983
2784.584642	181275.330902	56.015988
2783.729642	181161.784549	56.020993
2783.083159	181056.918879	56.025997
2782.519309	180944.039324	56.031002
2781.949742	180834.188388	56.036007
2781.099282	180734.469346	56.041012
2780.803335	180604.210608	56.046017
2780.021277	180512.405917	56.051021
2779.316049	180394.436699	56.056026
2778.658337	180285.313454	56.061031
2777.980540	180185.949945	56.066036
2777.350778	180070.208398	56.071041
2776.760061	179966.748483	56.076045
2775.900444	179855.266959	56.081050
2775.162609	179750.393516	56.086055
2774.457322	179646.341970	56.091060
2774.056608	179526.342622	56.096065
2773.061245	179419.424729	56.101069
2772.414738	179328.466069	56.106074
2772.212354	179212.506531	56.111079
2771.314183	179098.082120	56.116084
2770.914298	178992.508322	56.121089
2769.791408	178882.101353	56.126093
2769.510054	178772.388163	56.131098
2768.754132	178669.288294	56.136103
2767.894386	178556.207546	56.141108
2767.253371	178454.463718	56.146113
2766.552905	178357.588400	56.151117
2766.140063	178235.330575	56.156122
2765.338741	178136.512946	56.161127
2764.744090	178024.065778	56.166132
2764.484565	177913.880757	56.171137
2763.275238	177797.308727	56.176141
2762.812545	177687.945081	56.181146
2762.116635	177581.073479	56.186151
2761.375150	177478.724697	56.191156
2760.665891	177356.376484	56.196161
2759.981078	177267.794136	56.201165
2759.334437	177145.818202	56.206170
2758.558202	177045.396583	56.211175
2757.744154	176930.850315	56.216180
2757.665720	176829.504676	56.221185
2756.282712	176729.332561	56.226189
2755.652438	176619.553113	56.231194
2755.174957	176511.339625	56.236199
2754.411883	176421.715818	56.241204
2753.989102	176307.694380	56.246209
2753.188391	176202.432804	56.251213
2752.723644	176088.723874	56.256218
2752.217298	175996.071415	56.261223
2751.535974	175892.877605	56.266228
2750.952388	175786.323553	56.271233
2750.363284	175676.858077	56.276237
2749.622056	175556.059243	56.281242
2748.907940	175452.452026	56.286247
2748.082309	175333.625887	56.291252
2747.604303	175223.749756	56.296257
2746.791047	175127.535822	56.301261
2746.439558	175012.667288	56.306266
2745.664697	174896.505266	56.311271
2744.979141	174796.647138	56.316276
2744.442951	174679.722987	56.321281
2743.475722	174581.906788	56.326285
2742.871697	174464.408962	56.331290
2742.357094	174361.777680	56.336295
2741.355733	174258.066401	56.341300
2740.990836	174141.612690	56.346305
2740.136200	174041.757779	56.351309
2739.766630	173927.378490	56.356314
2739.084894	173822.409489	56.361319
2738.187812	173714.219049	56.366324
2737.924791	173598.780941	56.371329
2736.859722	173495.806655	56.376333
2736.078283	173385.945449	56.381338
2735.507813	173279.052559	56.386343
2734.731277	173171.798341	56.391348
2733.994463	173063.876793	56.396353
2733.412369	172962.709627	56.401357
2733.016732	172856.540531	56.406362
2732.196976	172755.284362	56.411367
2731.647354	172656.923456	56.416372
2730.913840	172536.514021	56.421377
2730.050352	172432.009880	56.426381
2729.568589	172323.553961	56.431386
2728.760930	172217.159340	56.436391
2728.043588	172117.999701	56.441396
2727.393511	172007.129545	56.446401
2727.202628	171897.064471	56.451405
2726.398424	171794.854494	56.456410
2725.416772	171694.046373	56.461415
2724.956208	171578.556423	56.466420
2724.162041	171476.193080	56.471425
2723.498597	171378.718178	56.476429
2722.703831	171268.508896	56.481434
2722.428333	171153.245232	56.486439
2721.549456	171059.620424	56.491444
2721.082322	170950.975226	56.496449
2720.091374	170843.646867	56.501453
2719.282790	170738.121180	56.506458
2719.140700	170638.708850	56.511463
2718.142522	170527.325766	56.516468
2717.872841	170407.650580	56.521473
2716.915078	170318.351117	56.526477
2716.165926	170214.254459	56.531482
2715.513510	170107.027119	56.536487
2715.106469	170007.582076	56.541492
2714.675943	169896.123610	56.546497
2713.797221	169782.930680	56.551501
2713.028965	169675.239653	56.556506
2712.424630	169580.366846	56.561511
2711.599844	169459.383693	56.566516
2711.063861	169358.663652	56.571521
2710.202691	169256.494826	56.576525
2709.628897	169154.827564	56.581530
2709.170810	169036.305542	56.586535
2708.575100	168939.042248	56.591540
2707.849313	168836.573336	56.596545
2707.578334	168717.653886	56.601549
2706.447131	168611.307707	56.606554
2705.744100	168505.695131	56.611559
2705.027304	168397.770657	56.616564
2704.776867	168289.073219	56.621569
2704.112655	168181.649681	56.626573
2703.431015	168076.212938	56.631578
2702.732619	167959.220135	56.636583
2702.017846	167850.762819	56.641588
2701.316050	167738.933990	56.646593
2700.434811	167637.840849	56.651597
2699.766356	167526.236259	56.656602
2699.070794	167423.143295	56.661607
2698.172152	167317.755763	56.666612
2698.086511	167203.631055	56.671617
2697.093152	167109.627150	56.676621
2696.435896	166991.728005	56.681626
2695.892311	166888.854035	56.686631
2695.194002	166790.582539	56.691636
2694.804009	166668.547591	56.696641
2693.770960	166572.097185	56.701645
2693.512031	166462.528977	56.706650
2692.581972	166342.182824	56.711655
2692.006234	166258.618016	56.716660
2691.477566	166135.678540	56.721665
2690.686030	166041.556343	56.726669
2689.818855	165921.773788	56.731674
2689.324290	165823.574290	56.736679
2688.227049	165702.341181	56.741684
2687.932572	165609.082282	56.746689
2687.160920	165496.139561	56.751693
2686.563783	165390.557131	56.756698
2686.104842	165275.976132	56.761703
2685.444968	165175.286919	56.766708
2684.814288	165068.566354	56.771713
2684.395192	164956.243339	56.776717
2683.389367	164858.750441	56.781722
2682.903449	164740.602430	56.786727
2682.133132	164641.966587	56.791732
2681.688493	164518.892026	56.796737
2680.917337	164412.144761	56.801741
2680.374937	164300.695189	56.806746
2680.002766	164191.812826	56.811751
2678.927207	164086.068354	56.816756
2678.664323	163959.381291	56.821761
2677.731228	163855.077123	56.826765
2677.147295	163739.579830	56.831770
2676.086633	163619.441276	56.836775
2675.779993	163507.092179	56.841780
2674.798217	163400.190525	56.846785
2674.000303	163300.240362	56.851789
2673.705350	163190.229878	56.856794
2673.466891	163074.768971	56.861799
2672.068510	162960.458488	56.866804
2671.774810	162852.940865	56.871809
2671.090614	162728.486294	56.876813
2670.535115	162624.430995	56.881818
2669.772303	162513.288827	56.886823
2669.047959	162395.211636	56.891828
2668.127616	162277.331167	56.896833
2667.305944	162177.756592	56.901837
2667.017297	162059.471623	56.906842
2666.217144	161946.086723	56.911847
2665.439244	161847.828397	56.916852
2664.864873	161739.850004	56.921857
2664.465563	161637.730781	56.926861
2663.528698	161528.030497	56.931866
2663.267199	161406.819174	56.936871
2662.554712	161300.262521	56.941876
2662.028480	161182.602930	56.946881
2661.041360	161080.832704	56.951885
2660.506187	160961.077486	56.956890
2659.903137	160855.267655	56.961895
2658.748542	160741.192634	56.966900
2658.385423	160631.226230	56.971905
2657.788688	160513.986861	56.976909
2656.888133	160398.181792	56.981914
2655.990184	160295.967434	56.986919
2655.493345	160188.909558	56.991924
2655.271066	160081.554239	56.996929
2654.577799	159982.257881	57.001933
2653.728049	159860.255104	57.006938
2653.345171	159745.819486	57.011943
2652.487257	159636.824503	57.016948
2651.934985	159517.369295	57.021953
2651.150290	159403.252719	57.026957
2650.312385	159291.509590	57.031962
2649.941293	159188.032663	57.036967
2648.866674	159081.883340	57.041972
2648.450796	158964.887459	57.046977
2647.591119	158861.120229	57.051981
2646.921642	158759.649647	57.056986
2646.600373	158638.292041	57.061991
2645.633778	158533.779952	57.066996
2645.103014	158440.005042	57.072001
2644.659205	158313.392154	57.077005
2643.748682	158202.820888	57.082010
2643.240813	158096.279676	57.087015
2642.108082	157984.994261	57.092020
2641.592284	157878.582101	57.097025
2641.167067	157770.770245	57.102029
2640.429654	157655.228104	57.107034
2640.268585	157544.069840	57.112039
2639.247782	157444.146138	57.117044
2638.574922	157320.954692	57.122049
2638.081648	157215.494442	57.127053
2637.286823	157103.090498	57.132058
2636.497342	156996.368478	57.137063
2635.843773	156883.408957	57.142068
2635.238917	156759.242620	57.147073
2634.404178	156663.524882	57.152077
2633.629631	156559.242599	57.157082
2633.402068	156448.072992	57.162087
2632.716766	156334.395721	57.167092
2632.256719	156213.055927	57.172097
2631.701055	156104.519963	57.177101
2630.893350	155983.528444	57.182106
2630.484599	155869.605516	57.187111
2629.453982	155759.010308	57.192116
2628.949120	155641.747444	57.197121
2628.450915	155530.051682	57.202125
2627.455278	155416.553767	57.207130
2626.865369	155294.843763	57.212135
2626.222441	155179.612819	57.217140
2625.633362	155054.776486	57.222145
2624.891097	154946.731411	57.227149
2624.056625	154839.451270	57.232154
2623.696670	154727.367623	57.237159
2622.944958	154601.109631	57.242164
2622.360058	154483.736353	57.247169
2621.568442	154366.002187	57.252173
2620.692441	154260.967667	57.257178
2620.537773	154147.048426	57.262183
2619.723674	154029.598650	57.267188
2618.973049	153914.249283	57.272193
2618.405813	153793.926634	57.277197
2617.867785	153673.790456	57.282202
2617.375687	153541.648234	57.287207
2616.426447	153433.094259	57.292212
2615.682055	153328.359593	57.297217
2614.863115	153203.274225	57.302221
2613.995100	153089.967341	57.307226
2613.472321	152973.669948	57.312231
2612.804139	152859.887309	57.317236
2612.251635	152747.955206	57.322241
2611.642030	152634.926701	57.327245
2610.881406	152515.401960	57.332250
2610.342974	152409.074159	57.337255
2609.615222	152295.455427	57.342260
2609.086221	152178.602550	57.347265
2608.303327	152065.933923	57.352269
2607.603092	151951.320602	57.357274
2606.914221	151830.134625	57.362279
2605.895822	151727.609208	57.367284
2605.604430	151609.360700	57.372289
2604.712468	151503.651092	57.377293
2604.197638	151393.522474	57.382298
2603.717478	151276.550674	57.387303
2602.938002	151170.646376	57.392308
2602.403675	151048.142372	57.397313
2602.130654	150938.370983	57.402317
2600.837407	150827.427071	57.407322
2600.801369	150703.409180	57.412327
2599.923004	150584.660017	57.417332
2599.538386	150461.880296	57.422337
2598.405121	150348.256317	57.427341
2597.823078	150237.379665	57.432346
2597.269016	150112.899587	57.437351
2596.363624	150001.973299	57.442356
2595.826140	149877.415241	57.447361
2595.317514	149761.076169	57.452365
2594.222552	149657.056970	57.457370
2593.812679	149544.414208	57.462375
2593.161446	149423.892114	57.467380
2592.415835	149296.191922	57.472385
2591.881683	149191.017777	57.477389
2591.154932	149077.931193	57.482394
2590.590646	148950.216351	57.487399
2589.926533	148842.979624	57.492404
2589.236716	148720.254882	57.497409
2588.672278	148613.435240	57.502413
2588.117907	148490.740751	57.507418
2587.368585	148393.114367	57.512423
2587.007207	148207.658763	57.517428
2586.347505	148076.874251	57.522433
2585.553352	147955.211107	57.527437
2584.710125	147837.203626	57.532442
2584.236207	147714.029148	57.537447
2583.335877	147607.469438	57.542452
2582.845477	147476.114093	57.547457
2582.316078	147355.046725	57.552461
2581.636011	147240.141923	57.557466
2581.036832	147107.178648	57.562471
2579.919019	146996.054980	57.567476
2579.737218	146856.405517	57.572481
2578.938645	146760.901547	57.577485
2578.315779	146628.185499	57.582490
2577.298826	146498.175774	57.587495
2576.751904	146391.182914	57.592500
2576.290758	146275.611522	57.597505
2575.615386	146155.524995	57.602509
2574.907072	146033.423565	57.607514
2574.262804	145912.519723	57.612519
2573.589017	145789.422546	57.617524
2572.689369	145680.073489	57.622529
2571.907670	145552.190751	57.627533
2571.259535	145440.299227	57.632538
2570.938122	145327.644695	57.637543
2570.277897	145210.304273	57.642548
2569.423787	145053.893498	57.647553
2568.931986	144969.173312	57.652557
2568.142674	144819.704521	57.657562
2567.665711	144718.767808	57.662567
2566.731944	144589.858391	57.667572
2566.356819	144475.398284	57.672577
2565.406781	144379.290221	57.677581
2564.868974	144236.049131	57.682586
2564.217905	144112.395862	57.687591
2563.512458	144010.455665	57.692596
2562.817734	143879.135074	57.697601
2562.183619	143772.978278	57.702605
2561.768070	143649.721582	57.707610
2560.984048	143522.965798	57.712615
2560.449720	143402.638826	57.717620
2559.671341	143296.125326	57.722625
2558.809361	143160.513943	57.727629
2558.303819	143042.255043	57.732634
2557.433404	142917.561249	57.737639
2556.810725	142819.144373	57.742644
2556.254626	142681.161302	57.747649
2555.574048	142581.648883	57.752653
2555.111540	142455.761438	57.757658
2554.472080	142325.861873	57.762663
2553.648384	142206.119132	57.767668
2553.055615	142091.816744	57.772673
2552.491526	141985.985411	57.777677
2551.679048	141857.398609	57.782682
2551.291070	141728.084351	57.787687
2550.410316	141604.121827	57.792692
2549.973497	141476.252187	57.797697
2549.226554	141367.250028	57.802701
2548.671701	141231.814558	57.807706
2547.968386	141105.513447	57.812711
2547.236410	140987.616061	57.817716
2546.378736	140857.503241	57.822721
2546.063173	140727.965778	57.827725
2545.359964	140617.167866	57.832730
2544.709507	140490.251075	57.837735
2543.942838	140368.651522	57.842740
2543.454084	140240.071122	57.847745
2542.966923	140103.448365	57.852749
2541.868572	139999.017338	57.857754
2541.616091	139861.494514	57.862759
2540.614257	139735.945265	57.867764
2540.039793	139619.654582	57.872769
2539.259124	139495.545120	57.877773
2538.430784	139379.244786	57.882778
2537.915225	139256.911161	57.887783
2537.303079	139133.310120	57.892788
2536.567381	139004.888511	57.897793
2536.016244	138889.562570	57.902797
2535.197500	138738.743489	57.907802
2534.678449	138635.483232	57.912807
2534.090459	138509.708402	57.917812
2533.504598	138373.833390	57.922817
2533.016303	138277.150633	57.927821
2532.160921	138121.830281	57.932826
2531.499726	137998.788044	57.937831
2530.794068	137898.710700	57.942836
2530.246101	137748.603326	57.947841
2529.309459	137620.740454	57.952845
2528.396857	137532.143956	57.957850
2527.877755	137381.474879	57.962855
2527.167911	137272.761302	57.967860
2526.991400	137141.527720	57.972865
2526.404242	137022.682967	57.977869
2525.720353	136896.549087	57.982874
2525.284391	136753.772093	57.987879
2523.994155	136639.486784	57.992884
2523.416856	136505.727924	57.997889
2522.817565	136389.034655	58.002893
2521.837415	136262.137408	58.007898
2521.422365	136142.735388	58.012903
2520.883296	136015.489824	58.017908
2520.153550	135881.961247	58.022913
2519.455789	135770.647065	58.027917
2518.773770	135637.988603	58.032922
2518.234057	135524.871797	58.037927
2517.441372	135392.295516	58.042932
2516.926069	135273.471914	58.047937
2516.493325	135142.757962	58.052941
2515.702680	135009.611454	58.057946
2515.023358	134879.153731	58.062951
2514.102901	134761.971659	58.067956
2513.809180	134629.510346	58.072961
2513.233342	134503.623794	58.077965
2512.238583	134382.097847	58.082970
2511.762055	134253.338444	58.087975
2511.052814	134133.229153	58.092980
2510.504080	134010.071618	58.097985
2509.245933	133873.041132	58.102989
2508.755604	133763.962934	58.107994
2508.310664	133605.502142	58.112999
2507.452370	133509.274953	58.118004
2507.062627	133391.633279	58.123009
2506.549456	133250.892838	58.128013
2505.691266	133140.770190	58.133018
2505.344826	132995.672999	58.138023
2504.511724	132870.063046	58.143028
2503.714010	132745.248292	58.148033
2503.373017	132600.037931	58.153037
2502.810014	132463.539161	58.158042
2502.176535	132351.910488	58.163047
2501.346252	132199.552151	58.168052
2500.301611	132078.717138	58.173057
2499.630470	131954.762247	58.178061
2499.097025	131818.528643	58.183066
2498.560886	131690.133220	58.188071
2497.491928	131592.421685	58.193076
2497.176182	131445.257151	58.198081
2496.485175	131322.667281	58.203085
2495.678160	131197.644899	58.208090
2495.307811	131047.557000	58.213095
2494.535406	130952.645856	58.218100
2493.945631	130802.378117	58.223105
2493.377843	130665.698278	58.228109
2492.715583	130558.361669	58.233114
2492.276935	130414.232252	58.238119
2491.146862	130275.395297	58.243124
2490.622362	130171.315274	58.248129
2490.116530	130018.320371	58.253133
2489.244322	129893.352248	58.258138
2488.594242	129781.977732	58.263143
2488.265575	129643.804367	58.268148
2487.199697	129509.050783	58.273153
2486.779807	129386.553435	58.278157
2486.022603	129236.180953	58.283162
2485.130358	129137.865755	58.288167
2484.381028	128978.704479	58.293172
2484.284205	128872.542117	58.298177
2483.757857	128722.542252	58.303181
2482.653125	128594.200375	58.308186
2482.450083	128469.539021	58.313191
2481.709792	128324.845923	58.318196
2481.019851	128185.149541	58.323201
2480.101425	128076.542292	58.328205
2479.646919	127929.634223	58.333210
2478.953708	127779.907236	58.338215
2477.982556	127684.314862	58.343220
2477.761655	127522.957311	58.348225
2476.624761	127394.664229	58.353229
2475.688911	127262.491807	58.358234
2474.985446	127158.972188	58.363239
2474.710866	127028.943958	58.368244
2474.160201	126895.226380	58.373249
2473.681758	126757.116616	58.378253
2472.619546	126635.761991	58.383258
2472.247118	126507.707496	58.388263
2471.459576	126372.188590	58.393268
2471.207120	126248.040447	58.398273
2470.367127	126106.981518	58.403277
2469.415250	125984.164583	58.408282
2469.071703	125829.871906	58.413287
2468.359536	125722.092181	58.418292
2467.743316	125567.094967	58.423297
2466.984388	125430.153929	58.428301
2466.112215	125320.394714	58.433306
2465.615424	125186.384931	58.438311
2464.761128	125045.803661	58.443316
2464.327972	124922.909325	58.448321
2463.715648	124782.672038	58.453325
2462.715686	124649.024055	58.458330
2462.186060	124524.153135	58.463335
2461.776689	124397.117674	58.468340
2461.081281	124254.635963	58.473345
2460.299886	124143.051275	58.478349
2459.437396	123990.565670	58.483354
2459.384330	123868.161941	58.488359
2458.722016	123726.820641	58.493364
2457.806339	123581.177467	58.498369
2457.357478	123467.117534	58.503373
2456.430035	123309.312894	58.508378
2455.646182	123197.123039	58.513383
2455.037555	123048.856406	58.518388
2454.247327	122916.961547	58.523393
2453.908124	122784.919663	58.528397
2453.066384	122649.199560	58.533402
2452.973542	122496.435432	58.538407
2451.991374	122393.473527	58.543412
2451.339899	122237.650430	58.548417
2450.897037	122090.162821	58.553421
2450.031761	121963.884190	58.558426
2449.597998	121830.122505	58.563431
2448.727219	121685.942809	58.568436
2448.039568	121537.455912	58.573441
2447.584373	121416.803250	58.578445
2446.597078	121267.920970	58.583450
2446.018180	121127.189765	58.588455
2445.339916	121012.008645	58.593460
2444.548196	120859.974223	58.598465
2444.112107	120722.269805	58.603469
2443.027132	120582.675579	58.608474
2442.806008	120446.792259	58.613479
2441.729626	120321.697687	58.618484
2441.276829	120174.323970	58.623489
2440.770925	120064.293545	58.628493
2439.956017	119909.938513	58.633498
2439.574223	119786.875749	58.638503
2438.851138	119637.160995	58.643508
2437.861791	119509.625184	58.648513
2437.543264	119368.214668	58.653517
2436.675494	119220.239234	58.658522
2436.229192	119102.433421	58.663527
2435.441178	118934.253941	58.668532
2434.732057	118833.421070	58.673537
2433.768005	118680.112661	58.678541
2433.282627	118532.156716	58.683546
2432.848668	118399.421943	58.688551
2431.699772	118289.335927	58.693556
2431.382483	118141.704704	58.698561
2430.802888	117992.776533	58.703565
2430.216543	117874.078096	58.708570
2429.438614	117716.930933	58.713575
2428.680827	117607.395214	58.718580
2428.011843	117442.685103	58.723585
2427.524413	117315.378907	58.728589
2426.497856	117194.995115	58.733594
2426.218640	117039.074293	58.738599
2425.275606	116913.397459	58.743604
2425.022795	116778.719055	58.748609
2424.219631	116634.239340	58.753613
2423.081562	116510.372683	58.758618
2423.042476	116350.596872	58.763623
2421.593982	116243.391714	58.768628
2421.199807	116084.194344	58.773633
2420.328906	115969.269360	58.778637
2419.977808	115839.175168	58.783642
2419.309786	115684.961841	58.788647
2419.102264	115586.048903	58.793652
2417.795064	115426.683036	58.798657
2417.311350	115303.188221	58.803661
2416.531268	115144.438748	58.808666
2416.435833	115028.182815	58.813671
2415.529212	114883.697729	58.818676
2415.021724	114751.247457	58.823681
2414.039555	114620.637571	58.828685
2413.800656	114464.300916	58.833690
2413.290537	114345.848034	58.838695
2412.266729	114185.867519	58.843700
2411.192140	114059.724302	58.848705
2411.479362	113917.962317	58.853709
2410.368745	113770.183934	58.858714
2409.822641	113655.662268	58.863719
2409.251146	113511.506395	58.868724
2408.403374	113344.801305	58.873729
2408.142596	113225.387587	58.878733
2407.211888	113061.883502	58.883738
2406.465953	112942.732097	58.888743
2405.897816	112789.764596	58.893748
2404.846022	112654.790611	58.898753
2404.905111	112491.260284	58.903757
2403.750706	112396.800159	58.908762
2403.465219	112211.120461	58.913767
2402.305582	112090.242725	58.918772
2401.920567	111959.145921	58.923777
2401.128028	111804.436770	58.928781
2400.250071	111694.806185	58.933786
2400.075574	111535.920149	58.938791
2399.460401	111382.416666	58.943796
2398.480423	111245.560533	58.948801
2398.064198	111096.793167	58.953805
2396.994152	110968.335931	58.958810
2396.540545	110836.227911	58.963815
2396.051349	110689.943142	58.968820
2395.692765	110537.578235	58.973825
2394.877060	110391.169323	58.978829
2394.010076	110244.991517	58.983834
2393.402898	110103.792884	58.988839
2392.444739	109961.445022	58.993844
2391.922184	109820.748608	58.998849
2391.277188	109679.387085	59.003853
2390.342058	109545.909202	59.008858
2390.047296	109391.840679	59.013863
2389.025794	109259.291819	59.018868
2388.363138	109121.597700	59.023873
2387.744965	108985.858055	59.028877
2387.342276	108844.761192	59.033882
2386.917798	108688.572927	59.038887
2386.161976	108555.237028	59.043892
2385.028721	108430.876871	59.048897
2384.811195	108275.388165	59.053901
2384.079830	108130.007396	59.058906
2383.414675	108003.639921	59.063911
2382.890115	107842.307978	59.068916
2382.057639	107707.079009	59.073921
2381.375160	107570.120188	59.078925
2380.821315	107416.314668	59.083930
2380.244986	107289.708426	59.088935
2379.802059	107139.027874	59.093940
2378.825717	106979.423024	59.098945
2378.040948	106839.426317	59.103949
2377.151126	106713.050471	59.108954
2377.114046	106548.439403	59.113959
2376.055417	106406.096646	59.118964
2375.461946	106278.013774	59.123969
2375.429276	106110.473739	59.128973
2374.238282	105977.551030	59.133978
2373.592701	105839.105235	59.138983
2372.788170	105664.762359	59.143988
2371.873768	105564.447373	59.148993
2371.391383	105409.888394	59.153997
2370.573924	105276.396466	59.159002
2370.476402	105121.543593	59.164007
2369.578715	104969.692605	59.169012
2368.704869	104834.200926	59.174017
2368.206490	104697.026342	59.179021
2367.310223	104556.794245	59.184026
2367.015499	104413.396984	59.189031
2366.096017	104260.253425	59.194036
2365.723762	104106.903556	59.199041
2365.275710	103971.577694	59.204045
2364.117404	103830.509616	59.209050
2363.920986	103678.098954	59.214055
2363.093454	103529.341990	59.219060
2362.122304	103398.314784	59.224065
2361.733428	103245.810553	59.229069
2360.690677	103110.228668	59.234074
2360.268332	102960.345285	59.239079
2359.741422	102814.615610	59.244084
2359.256794	102667.287847	59.249089
2358.476260	102536.070294	59.254093
2357.290398	102394.380836	59.259098
2357.231222	102236.426052	59.264103
2356.336474	102089.649070	59.269108
2355.478055	101959.043406	59.274113
2355.275326	101810.604276	59.279117
2354.257642	101653.369986	59.284122
2353.655200	101519.694001	59.289127
2352.904595	101378.163729	59.294132
2352.380803	101223.391409	59.299137
2351.412885	101078.858932	59.304141
2350.421707	100957.712507	59.309146
2350.144044	100791.042041	59.314151
2349.218627	100676.451950	59.319156
2348.729357	100528.110845	59.324161
2348.142318	100401.746228	59.329165
2347.331535	100267.133647	59.334170
2346.977650	100111.663099	59.339175
2346.345843	99973.198973	59.344180
2345.667913	99838.421938	59.349185
2345.145270	99700.075346	59.354189
2344.813490	99547.973212	59.359194
2343.957067	99400.109863	59.364199
2343.509903	99249.214119	59.369204
2342.305769	99124.197553	59.374209
2342.047637	98948.581242	59.379213
2341.165480	98822.253059	59.384218
2340.544655	98670.323079	59.389223
2339.589484	98520.990524	59.394228
2339.034399	98378.134736	59.399233
2338.287254	98234.631639	59.404237
2337.420568	98098.645271	59.409242
2336.731312	97971.117839	59.414247
2336.312469	97811.081208	59.419252
2335.484179	97679.391436	59.424257
2335.327099	97539.921721	59.429261
2334.573614	97410.435135	59.434266
2334.137054	97257.273962	59.439271
2333.363028	97107.712652	59.444276
2332.705021	96944.117643	59.449281
2332.224429	96804.602264	59.454285
2330.978203	96668.595844	59.459290
2330.779093	96514.761480	59.464295
2329.951493	96373.344077	59.469300
2329.499511	96230.466415	59.474305
2328.695642	96071.841269	59.479309
2328.048385	95928.844273	59.484314
2327.388041	95795.065021	59.489319
2326.488766	95646.135724	59.494324
2325.596155	95493.363224	59.499329
2324.966424	95346.942573	59.504333
2324.294010	95225.858491	59.509338
2323.819499	95061.575816	59.514343
2323.143302	94932.497058	59.519348
2322.819147	94782.068111	59.524353
2322.373651	94634.405311	59.529357
2321.396327	94497.012297	59.534362
2320.759488	94342.666093	59.539367
2319.976133	94195.516352	59.544372
2319.384166	94049.998678	59.549377
2318.799720	93889.343956	59.554381
2318.105410	93770.896544	59.559386
2317.265273	93609.276118	59.564391
2316.289182	93473.201864	59.569396
2315.713502	93313.653282	59.574401
2315.042250	93204.628235	59.579405
2314.516340	93028.998988	59.584410
2314.150361	92910.764084	59.589415
2313.443296	92754.239686	59.594420
2313.017003	92606.263902	59.599425
2312.485739	92485.590836	59.604429
2311.445687	92312.870519	59.609434
2310.938775	92173.419904	59.614439
2310.657418	91996.295335	59.619444
2309.580736	91880.974934	59.624449
2309.130251	91717.854494	59.629453
2308.194386	91559.022443	59.634458
2307.586552	91436.395310	59.639463
2306.818182	91267.305006	59.644468
2305.935987	91138.319041	59.649473
2305.471324	90978.598535	59.654477
2304.722994	90836.607749	59.659482
2304.272819	90702.394698	59.664487
2303.696877	90547.710263	59.669492
2302.931749	90400.595595	59.674497
2302.328603	90249.056060	59.679501
2301.298409	90117.106963	59.684506
2300.903890	89970.386583	59.689511
2300.059566	89817.804111	59.694516
2299.597251	89674.545530	59.699521
2299.322556	89522.343968	59.704525
2298.415457	89371.245484	59.709530
2297.579977	89223.395455	59.714535
2297.267366	89083.077814	59.719540
2296.213777	88924.835170	59.724545
2295.577296	88763.928191	59.729549
2295.015094	88625.954461	59.734554
2294.489072	88484.362193	59.739559
2293.679175	88327.137681	59.744564
2292.601394	88176.258453	59.749569
2292.542920	88039.216599	59.754573
2291.519605	87910.709596	59.759578
2291.167910	87740.991040	59.764583
2290.704888	87585.751926	59.769588
2289.620328	87448.933599	59.774593
2289.318546	87293.493519	59.779597
2288.393741	87146.870029	59.784602
2287.825088	86998.752030	59.789607
2287.119410	86862.232363	59.794612
2286.531520	86696.451849	59.799617
2285.980064	86537.899884	59.804621
2285.016184	86399.332174	59.809626
2284.509793	86258.657950	59.814631
2284.086321	86105.965269	59.819636
2282.990578	85945.608626	59.824641
2282.504761	85816.223889	59.829645
2281.851091	85630.918942	59.834650
2281.383680	85503.618697	59.839655
2280.601556	85336.294821	59.844660
2279.758754	85209.727786	59.849665
2279.384622	85044.731240	59.854669
2278.717276	84885.170390	59.859674
2277.696414	84763.743266	59.864679
2277.492656	84567.207482	59.869684
2276.632857	84462.059506	59.874689
2276.028987	84299.355397	59.879693
2275.594060	84133.488190	59.884698
2274.596969	84001.679215	59.889703
2274.052000	83820.283684	59.894708
2273.041700	83706.010688	59.899713
2272.902347	83519.894713	59.904718
2272.119645	83388.492918	59.909722
2271.697037	83229.577619	59.914727
2270.929073	83069.615446	59.919732
2269.843068	82934.018015	59.924737
2269.528360	82745.204967	59.929742
2268.774126	82634.370461	59.934746
2267.852492	82449.490848	59.939751
2267.181928	82310.516799	59.944756
2266.770272	82194.959222	59.949761
2266.043600	82003.068254	59.954766
2265.118108	81864.638291	59.959770
2264.497590	81694.801604	59.964775
2264.191407	81583.603740	59.969780
2263.592881	81397.306912	59.974785
2262.776108	81272.686108	59.979790
2261.885741	81091.685863	59.984794
2261.400835	80971.678690	59.989799
2260.863361	80813.985094	59.994804
2259.887027	80649.669954	59.999809
2259.271777	80513.715747	60.004814
2258.600665	80360.673097	60.009818
2258.127448	80212.365850	60.014823
2257.408571	80063.052978	60.019828
2256.604920	79913.000500	60.024833
2256.034056	79745.396254	60.029838
2255.168474	79619.918607	60.034842
2254.623687	79463.991844	60.039847
2253.920067	79310.943117	60.044852
2253.188212	79164.484136	60.049857
2252.931767	79011.677225	60.054862
2252.315960	78867.888814	60.059866
2251.742037	78723.676535	60.064871
2250.984182	78569.203465	60.069876
2250.179517	78412.020513	60.074881
2249.904562	78251.700462	60.079886
2248.905783	78095.951135	60.084890
2248.619621	77947.624205	60.089895
2247.816624	77789.812106	60.094900
2246.898690	77641.403837	60.099905
2246.270780	77479.808809	60.104910
2245.654473	77330.594587	60.109914
2245.069713	77176.022217	60.114919
2244.432079	77008.583995	60.119924
2243.630898	76871.156342	60.124929
2243.095255	76714.571086	60.129934
2242.035130	76570.736253	60.134938
2242.063792	76409.096283	60.139943
2241.074595	76250.166140	60.144948
2240.369463	76102.660419	60.149953
2239.794013	75942.140087	60.154958
2238.816451	75789.946870	60.159962
2238.342582	75645.886233	60.164967
2237.738792	75484.639062	60.169972
2237.031772	75327.546827	60.174977
2236.425845	75168.925538	60.179982
2235.880177	75025.089799	60.184986
2235.260100	74867.949342	60.189991
2234.435865	74695.662393	60.194996
2233.699071	74553.140131	60.200001
2233.110427	74410.791784	60.205006
2232.702745	74243.238627	60.210010
2232.003672	74080.395943	60.215015
2231.054515	73950.785188	60.220020
2230.433248	73794.242511	60.225025
2230.018985	73629.812500	60.230030
2229.016174	73477.317699	60.235034
2228.553629	73317.414923	60.240039
2227.824984	73161.356700	60.245044
2227.195608	73026.487424	60.250049
2226.443115	72846.051778	60.255054
2225.411241	72713.928168	60.260058
2225.428460	72541.564318	60.265063
2224.793807	72391.002265	60.270068
2223.563131	72246.896049	60.275073
2223.299321	72088.529983	60.280078
2222.535514	71934.013645	60.285082
2221.975960	71780.752052	60.290087
2221.228980	71635.693041	60.295092
2220.393040	71459.464084	60.300097
2219.640989	71328.344192	60.305102
2219.253082	71155.245821	60.310106
2218.593889	70997.622644	60.315111
2218.320069	70859.436809	60.320116
2217.213455	70697.167888	60.325121
2216.637266	70531.718711	60.330126
2215.956486	70398.091661	60.335130
2215.390689	70238.743163	60.340135
2214.816655	70073.164483	60.345140
2213.927463	69924.663180	60.350145
2213.424896	69766.233261	60.355150
2212.446307	69599.721966	60.360154
2211.716583	69452.947120	60.365159
2211.197598	69314.418329	60.370164
2210.376896	69133.932416	60.375169
2209.899252	69006.394768	60.380174
2208.786533	68819.807975	60.385178
2208.463139	68706.245349	60.390183
2207.808937	68534.295378	60.395188
2207.206500	68388.730727	60.400193
2206.469993	68229.203992	60.405198
2205.384551	68101.781334	60.410202
2205.172530	67936.771340	60.415207
2204.795701	67777.545930	60.420212
2204.063204	67635.674573	60.425217
2203.734388	67476.697347	60.430222
2202.937604	67326.187186	60.435226
2201.867663	67164.100130	60.440231
2201.280900	67009.809872	60.445236
2200.501030	66850.542008	60.450241
2199.846447	66698.582897	60.455246
2198.862638	66563.864919	60.460250
2198.554281	66409.475129	60.465255
2197.975554	66256.136388	60.470260
2196.825578	66112.455228	60.475265
2196.620880	65946.989233	60.480270
2195.924110	65799.100051	60.485274
2195.533533	65650.777142	60.490279
2194.932271	65502.289320	60.495284
2193.733438	65342.229643	60.500289
2193.646502	65187.982340	60.505294
2192.750591	65027.459293	60.510298
2192.091774	64872.630831	60.515303
2191.379849	64719.053191	60.520308
2190.841088	64558.239962	60.525313
2190.154625	64411.632643	60.530318
2189.645156	64265.707583	60.535322
2188.903517	64092.927717	60.540327
2188.361155	63941.957278	60.545332
2187.466095	63793.931406	60.550337
2186.821676	63632.930609	60.555342
2186.136594	63488.011324	60.560346
2185.526555	63331.069587	60.565351
2185.190232	63166.724935	60.570356
2184.304762	63005.454262	60.575361
2183.581112	62841.028238	60.580366
2183.062997	62714.488458	60.585370
2182.385392	62531.455254	60.590375
2181.936205	62382.821969	60.595380
2181.207960	62229.124556	60.600385
2180.985456	62059.509932	60.605390
2179.753496	61903.087058	60.610394
2179.293081	61741.544462	60.615399
2178.855245	61567.625082	60.620404
2177.631654	61419.138054	60.625409
2177.215513	61255.395648	60.630414
2176.339760	61100.081553	60.635418
2175.611477	60936.518061	60.640423
2175.158346	60792.035325	60.645428
2174.194617	60632.206011	60.650433
2174.053963	60475.194556	60.655438
2172.713950	60314.202603	60.660442
2172.235790	60140.302829	60.665447
2172.040292	59994.671140	60.670452
2170.877973	59842.021215	60.675457
2170.250322	59679.465652	60.680462
2169.713487	59522.762433	60.685466
2169.191228	59358.322244	60.690471
2168.646439	59211.185251	60.695476
2167.989641	59050.402846	60.700481
2167.108692	58896.212542	60.705486
2166.457985	58738.688869	60.710490
2165.510885	58574.357814	60.715495
2165.385856	58422.387412	60.720500
2164.407517	58259.874552	60.725505
2163.688563	58118.471024	60.730510
2163.104128	57952.866222	60.735514
2162.265986	57795.614501	60.740519
2161.926342	57632.686156	60.745524
2160.956838	57478.660946	60.750529
2160.748520	57318.816204	60.755534
2159.533657	57159.892100	60.760538
2158.992948	57008.518289	60.765543
2158.571654	56849.584905	60.770548
2157.877014	56696.342323	60.775553
2157.204912	56535.150603	60.780558
2156.692987	56383.214028	60.785562
2156.195661	56216.642560	60.790567
2155.480138	56057.025308	60.795572
2154.661714	55899.296106	60.800577
2153.921639	55733.865679	60.805582
2153.210710	55582.900874	60.810586
2152.469225	55420.869161	60.815591
2151.974770	55252.473680	60.820596
2150.905727	55105.971564	60.825601
2150.601524	54945.529757	60.830606
2149.901740	54797.041173	60.835610
2149.228360	54631.002554	60.840615
2148.737287	54465.613719	60.845620
2148.057706	54315.841080	60.850625
2147.398934	54151.383562	60.855630
2146.697852	54012.375786	60.860634
2145.797749	53843.190631	60.865639
2145.174401	53679.953194	60.870644
2144.261319	53535.438821	60.875649
2143.966022	53374.006366	60.880654
2143.154686	53218.761023	60.885658
2142.443029	53065.887010	60.890663
2141.859960	52903.381107	60.895668
2141.141377	52742.932711	60.900673
2140.956964	52573.756612	60.905678
2139.565560	52431.981633	60.910682
2139.372219	52279.456030	60.915687
2138.892053	52121.307254	60.920692
2137.927199	51966.150817	60.925697
2137.285201	51803.806541	60.930702
2136.861221	51650.952659	60.935706
2136.030728	51483.037808	60.940711
2135.728572	51328.297458	60.945716
2134.724714	51180.529049	60.950721
2134.461373	51005.017645	60.955726
2133.572706	50849.830286	60.960730
2132.861291	50686.709837	60.965735
2132.728592	50523.382002	60.970740
2132.056178	50361.033453	60.975745
2131.215906	50190.534836	60.980750
2130.281185	50035.959784	60.985754
2129.672144	49869.265088	60.990759
2129.234328	49694.404801	60.995764
2128.030054	49536.156435	61.000769
2127.799462	49370.909061	61.005774
2126.997719	49220.015024	61.010778
2126.296664	49054.981254	61.015783
2125.847069	48887.390998	61.020788
2124.964258	48724.682649	61.025793
2124.415884	48557.139652	61.030798
2123.478057	48404.240064	61.035802
2122.573768	48250.412774	61.040807
2122.219164	48071.714933	61.045812
2121.525897	47930.462803	61.050817
2121.045798	47759.250256	61.055822
2120.206007	47601.242863	61.060826
2119.730999	47436.662791	61.065831
2118.986292	47276.745290	61.070836
2118.365433	47115.588612	61.075841
2117.827613	46955.796194	61.080846
2116.934733	46807.195665	61.085850
2116.434223	46631.407648	61.090855
2115.743895	46469.549891	61.095860
2115.061236	46324.756855	61.100865
2114.415185	46151.932000	61.105870
2113.398055	45994.014620	61.110874
2112.732847	45837.763459	61.115879
2112.741703	45663.865329	61.120884
2111.643320	45519.366306	61.125889
2111.083290	45355.252528	61.130894
2110.255006	45185.537240	61.135898
2109.872018	45038.695747	61.140903
2109.060860	44871.719760	61.145908
2108.237950	44710.715290	61.150913
2107.546259	44551.004007	61.155918
2106.927030	44397.453048	61.160922
2106.178572	44232.753519	61.165927
2105.764888	44073.227057	61.170932
2105.029262	43913.408418	61.175937
2104.488746	43739.107457	61.180942
2103.381103	43591.928248	61.185946
2103.130913	43436.530918	61.190951
2102.447005	43273.803637	61.195956
2101.797124	43120.613541	61.200961
2101.098499	42954.017623	61.205966
2100.465688	42790.559426	61.210970
2099.949085	42637.409387	61.215975
2099.113239	42471.175102	61.220980
2098.673209	42310.473698	61.225985
2098.195003	42140.922375	61.230990
2097.298408	41985.099906	61.235994
2096.650289	41813.080611	61.240999
2096.197479	41648.697127	61.246004
2095.209337	41495.103974	61.251009
2094.625063	41317.371856	61.256014
2093.958700	41154.946375	61.261018
2093.208691	40999.590219	61.266023
2092.718607	40835.609362	61.271028
2091.717955	40669.851840	61.276033
2091.336977	40511.349140	61.281038
2090.417771	40354.343525	61.286042
2089.777434	40189.297093	61.291047
2089.057406	40024.709143	61.296052
2088.339822	39868.890155	61.301057
2087.693040	39706.149651	61.306062
2087.550493	39549.149940	61.311066
2086.567449	39397.297984	61.316071
2085.936357	39220.771255	61.321076
2085.332148	39067.716009	61.326081
2084.706378	38902.458409	61.331086
2083.990374	38748.653913	61.336090
2083.335503	38575.149111	61.341095
2082.932408	38405.333615	61.346100
2081.822163	38260.546484	61.351105
2081.422072	38094.914753	61.356110
2080.835860	37918.369155	61.361114
2079.707775	37768.236698	61.366119
2079.125571	37613.053958	61.371124
2078.538780	37466.696799	61.376129
2078.178183	37287.986471	61.381134
2077.256189	37132.253504	61.386138
2076.521151	36975.578698	61.391143
2076.125547	36812.530541	61.396148
2074.974056	36645.582813	61.401153
2074.683243	36477.698810	61.406158
2073.819662	36338.203023	61.411162
2073.287319	36164.856864	61.416167
2072.888324	36012.572792	61.421172
2072.230527	35849.839527	61.426177
2071.347453	35687.559267	61.431182
2070.659068	35531.301464	61.436186
2070.047612	35361.938502	61.441191
2069.635797	35202.927749	61.446196
2069.191260	35042.396971	61.451201
2068.521521	34880.966261	61.456206
2067.710672	34713.368941	61.461210
2066.929249	34538.585635	61.466215
2066.438037	34372.145303	61.471220
2065.698978	34204.227210	61.476225
2065.085418	34041.834836	61.481230
2064.371088	33878.837378	61.486234
2063.853704	33725.899159	61.491239
2063.258667	33549.789720	61.496244
2062.249697	33377.099663	61.501249
2061.883920	33211.319516	61.506254
2061.190218	33049.502664	61.511258
2060.374795	32877.702079	61.516263
2060.013687	32706.728765	61.521268
2058.920717	32554.802903	61.526273
2058.487136	32370.891427	61.531278
2058.004125	32218.882927	61.536282
2057.199023	32047.681905	61.541287
2056.509149	31877.619476	61.546292
2055.747183	31705.256904	61.551297
2055.281561	31535.021793	61.556302
2054.281002	31377.737049	61.561306
2053.486553	31217.230880	61.566311
2053.147554	31034.607087	61.571316
2052.030644	30902.854240	61.576321
2051.528145	30716.864354	61.581326
2050.687205	30558.914304	61.586330
2050.258610	30396.789126	61.591335
2049.683590	30244.679171	61.596340
2048.907602	30074.320434	61.601345
2048.107940	29908.688193	61.606350
2047.405819	29749.793318	61.611354
2046.887359	29591.760353	61.616359
2046.258784	29427.987552	61.621364
2045.438931	29271.793991	61.626369
2045.183940	29102.738819	61.631374
2044.508202	28943.150880	61.636378
2043.372728	28784.827099	61.641383
2042.891116	28626.445336	61.646388
2042.423549	28458.002497	61.651393
2041.535827	28290.669178	61.656398
2041.069746	28138.051308	61.661402
2040.388707	27970.336197	61.666407
2039.777586	27813.820203	61.671412
2038.882478	27644.627432	61.676417
2038.568980	27483.881045	61.681422
2037.519262	27326.545230	61.686426
2036.622850	27161.848083	61.691431
2036.152347	26995.405814	61.696436
2035.439544	26847.830297	61.701441
2034.855484	26683.997560	61.706446
2034.183204	26523.631224	61.711450
2033.875531	26364.049776	61.716455
2032.997465	26195.275453	61.721460
2031.968317	26043.608648	61.726465
2031.604237	25887.271157	61.731470
2030.991751	25727.916562	61.736474
2030.494429	25568.508153	61.741479
2029.795809	25407.600331	61.746484
2029.167016	25239.951918	61.751489
2028.568872	25078.199049	61.756494
2027.767263	24916.991066	61.761498
2026.811818	24760.251386	61.766503
2026.242819	24594.230258	61.771508
2025.147833	24440.870620	61.776513
2024.878693	24275.903713	61.781518
2024.023188	24138.462750	61.786522
2023.574622	23978.117953	61.791527
2022.895641	23816.798951	61.796532
2022.144233	23657.457804	61.801537
2022.137780	23493.791858	61.806542
2021.301450	23339.789768	61.811546
2020.724123	23179.580836	61.816551
2020.128770	23011.182183	61.821556
2019.148350	22855.009273	61.826561
2018.836347	22691.476668	61.831566
2018.171740	22527.735601	61.836570
2017.264398	22366.135919	61.841575
2016.605258	22200.978419	61.846580
2015.671231	22047.437874	61.851585
2015.218698	21878.835130	61.856590
2014.263041	21731.301209	61.861594
2013.930454	21553.509493	61.866599
2012.972226	21396.184411	61.871604
2011.946651	21248.726894	61.876609
2011.770370	21088.255977	61.881614
2011.368173	20929.992217	61.886618
2010.217409	20768.557263	61.891623
2009.963062	20596.195548	61.896628
2009.016599	20448.503218	61.901633
2008.265703	20296.006259	61.906638
2007.384033	20146.084009	61.911642
2006.614227	19991.113173	61.916647
2006.156090	19824.833900	61.921652
2005.792692	19692.526221	61.926657
2004.820583	19527.688003	61.931662
2004.075874	19377.072818	61.936666
2003.321721	19230.184466	61.941671
2002.769613	19081.119301	61.946676
2001.916469	18932.261616	61.951681
2001.572878	18759.378484	61.956686
2000.632995	18614.279922	61.961690
1999.539545	18477.031835	61.966695
1999.695151	18307.638722	61.971700
1998.685814	18178.734282	61.976705
1997.876490	18017.714797	61.981710
1997.455930	17883.622604	61.986714
1996.541119	17739.823210	61.991719
1996.282258	17583.704639	61.996724
1995.092978	17445.359160	62.001729
1994.054330	17296.777839	62.006734
1993.145060	17150.229535	62.011738
1992.544097	17019.217189	62.016743
1992.213229	16883.781252	62.021748
1991.143683	16768.354188	62.026753
1990.335299	16623.430360	62.031758
1989.522527	16491.390306	62.036762
1988.928834	16369.319994	62.041767
1988.060776	16251.314339	62.046772
1986.893517	16137.021611	62.051777
1986.081399	16012.746176	62.056782
1985.228117	15907.879645	62.061786
1984.607485	15798.637407	62.066791
1983.934977	15699.497301	62.071796
1982.858759	15599.271341	62.076801
1981.714227	15496.077084	62.081806
1981.045273	15401.541262	62.086810
1980.303472	15315.879208	62.091815
1979.313710	15217.969742	62.096820
1978.318158	15151.883281	62.101825
1977.647206	15066.630368	62.106830
1976.909541	14997.150422	62.111834
1976.149231	14915.908575	62.116839
1975.900718	14830.129208	62.121844
1975.083751	14761.260862	62.126849
1974.206289	14682.561727	62.131854
1973.573700	14619.542833	62.136858
1972.664639	14542.035544	62.141863
1972.086877	14471.302328	62.146868
1971.315696	14405.330074	62.151873
1970.873185	14331.430698	62.156878
1970.226312	14263.927491	62.161882
1969.497248	14197.049359	62.166887
1968.794969	14134.427570	62.171892
1968.204389	14075.049173	62.176897
1967.729189	14007.107201	62.181902
1966.874429	13936.429771	62.186906
1966.297549	13877.478499	62.191911
1965.816542	13796.554185	62.196916
1964.938674	13740.982948	62.201921
1964.399665	13663.891801	62.206926
1963.888507	13605.001386	62.211930
1963.157300	13537.690858	62.216935
1962.899816	13464.303433	62.221940
1961.560257	13391.638156	62.226945
1961.277784	13329.969082	62.231950
1960.523408	13262.295009	62.236954
1959.567236	13185.331311	62.241959
1959.346295	13129.435987	62.246964
1958.294667	13058.892418	62.251969
1957.955382	13010.466438	62.256974
1957.238893	12945.813825	62.261978
1956.341147	12877.489998	62.266983
1955.991863	12811.223102	62.271988
1954.979967	12747.141417	62.276993
1954.300585	12691.041117	62.281998
1953.882712	12629.713794	62.287002
1953.302830	12574.156239	62.292007
1952.596018	12503.596620	62.297012
1951.645150	12442.966808	62.302017
1951.074707	12373.122786	62.307022
1950.849960	12316.793687	62.312026
1949.783164	12266.847366	62.317031
1949.276564	12199.275705	62.322036
1948.716302	12138.303600	62.327041
1947.764517	12074.749237	62.332046
1947.469913	12005.361832	62.337050
1946.828493	11949.081099	62.342055
1946.353561	11885.218270	62.347060
1945.364765	11837.301559	62.352065
1944.659509	11765.074642	62.357070
1944.165719	11698.046856	62.362074
1943.218931	11642.535172	62.367079
1942.840483	11568.222699	62.372084
1942.492532	11514.315690	62.377089
1941.786051	11450.194958	62.382094
1941.021708	11374.765829	62.387098
1940.300517	11319.250297	62.392103
1939.589325	11239.874838	62.397108
1938.957181	11187.031192	62.402113
1938.116891	11142.035081	62.407118
1937.772261	11062.573962	62.412122
1936.587878	11010.422604	62.417127
1936.103774	10937.483596	62.422132
1935.712690	10884.218091	62.427137
1934.976953	10816.548526	62.432142
1934.130259	10753.282081	62.437146
1933.629822	10701.370794	62.442151
1933.214874	10635.719149	62.447156
1932.167022	10582.189701	62.452161
1931.945152	10506.618046	62.457166
1931.395447	10440.973253	62.462170
1930.418482	10381.529508	62.467175
1929.780154	10312.602481	62.472180
1928.972056	10249.423354	62.477185
1927.999253	10191.170696	62.482190
1927.174986	10135.077829	62.487194
1926.599950	10074.853513	62.492199
1926.359187	10018.586796	62.497204
1925.238874	9959.153670	62.502209
1924.653810	9903.555078	62.507214
1924.312749	9836.175999	62.512218
1923.633591	9788.700301	62.517223
1922.968020	9731.224347	62.522228
1922.103784	9671.005347	62.527233
1921.859082	9610.760828	62.532238
1921.196264	9554.732077	62.537242
1920.271819	9496.122957	62.542247
1919.993317	9422.363772	62.547252
1919.338524	9369.128920	62.552257
1918.603058	9316.131914	62.557262
1917.919053	9249.902598	62.562266
1917.151688	9183.007528	62.567271
1916.736706	9123.094950	62.572276
1915.865036	9059.265453	62.577281
1915.241320	8998.810583	62.582286
1914.654372	8942.403250	62.587290
1913.861695	8879.656227	62.592295
1913.389785	8812.029939	62.597300
1912.749072	8758.053042	62.602305
1911.929146	8704.244427	62.607310
1911.438905	8632.662282	62.612314
1910.663347	8573.884035	62.617319
1910.108564	8504.250315	62.622324
1909.233600	8452.326971	62.627329
1908.806579	8388.288934	62.632334
1908.471783	8313.977312	62.637338
1907.328768	8266.146578	62.642343
1906.914254	8191.260494	62.647348
1905.775255	8141.101508	62.652353
1905.034552	8079.976280	62.657358
1904.434946	8016.680780	62.662362
1903.697860	7962.533908	62.667367
1903.450041	7907.695819	62.672372
1902.450409	7854.288385	62.677377
1902.045973	7786.563333	62.682382
1901.555463	7736.608847	62.687386
1900.584649	7681.257636	62.692391
1900.122440	7611.457583	62.697396
1899.508577	7561.086239	62.702401
1898.644665	7489.414671	62.707406
1898.230746	7424.251417	62.712410
1897.573392	7372.577335	62.717415
1896.747981	7309.802668	62.722420
1895.952792	7262.856306	62.727425
1895.402968	7193.276431	62.732430
1894.866299	7138.620338	62.737434
1894.015695	7081.060895	62.742439
1893.361724	7013.091049	62.747444
1892.489739	6959.937924	62.752449
1891.735039	6903.957371	62.757454
1891.282671	6844.190817	62.762458
1890.437758	6796.712693	62.767463
1889.963270	6726.285320	62.772468
1889.204133	6675.805941	62.777473
1888.657500	6617.617109	62.782478
1888.257624	6558.610881	62.787482
1887.259780	6506.406207	62.792487
1886.646152	6447.060464	62.797492
1885.994316	6395.205907	62.802497
1885.510722	6341.713317	62.807502
1884.636088	6275.229317	62.812506
1883.970618	6217.290459	62.817511
1883.157781	6161.109758	62.822516
1882.283184	6112.639940	62.827521
1881.921686	6077.655818	62.832526
1881.784563	6021.932349	62.837530
1880.770669	5965.497196	62.842535
1880.351685	5900.635248	62.847540
1879.647647	5838.318438	62.852545
1878.891823	5780.422453	62.857550
1878.283056	5716.885012	62.862554
1877.482496	5656.470217	62.867559
1876.875318	5598.624700	62.872564
1876.227689	5547.938222	62.877569
1875.507957	5483.924063	62.882574
1875.072573	5417.180943	62.887578
1874.151202	5374.329733	62.892583
1873.614887	5307.453272	62.897588
1872.603392	5251.836022	62.902593
1871.922445	5210.597154	62.907598
1871.417851	5151.672313	62.912602
1871.023229	5097.234666	62.917607
1870.455588	5026.198397	62.922612
1869.417683	4980.144903	62.927617
1868.846251	4924.817892	62.932622
1868.425283	4866.135670	62.937626
1867.707240	4808.962328	62.942631
1867.173863	4755.096915	62.947636
1866.564320	4692.198918	62.952641
1865.955403	4628.357802	62.957646
1864.970001	4574.983613	62.962650
1864.141577	4523.315096	62.967655
1863.973120	4462.217263	62.972660
1862.889838	4405.980499	62.977665
1861.973728	4345.955374	62.982670
1861.667181	4304.328358	62.987674
1860.749547	4248.492577	62.992679
1860.368582	4189.591390	62.997684
1859.413437	4144.565279	63.002689
1858.842329	4087.572526	63.007694
1858.317598	4029.374641	63.012698
1857.532908	3978.078872	63.017703
1857.090194	3915.695580	63.022708
1856.303644	3865.984134	63.027713
1855.520810	3811.272175	63.032718
1855.063063	3753.635737	63.037722
1854.144570	3702.284887	63.042727
1853.594254	3642.441949	63.047732
1852.628399	3595.677102	63.052737
1852.031652	3539.629036	63.057742
1851.628823	3484.033045	63.062746
1850.494913	3448.670704	63.067751
1850.350792	3404.233402	63.072756
1849.621175	3345.465087	63.077761
1849.056979	3278.066006	63.082766
1848.598676	3237.484228	63.087770
1847.532783	3187.442474	63.092775
1846.874965	3114.472395	63.097780
1846.220472	3070.061933	63.102785
1845.715019	3025.038059	63.107790
1845.118146	2962.385200	63.112794
1844.337601	2914.884148	63.117799
1844.177331	2847.649248	63.122804
1843.350557	2804.882799	63.127809
1842.389342	2751.824492	63.132814
1841.871213	2689.948112	63.137818
1840.847695	2632.395661	63.142823
1840.385674	2581.316949	63.147828
1839.421568	2541.381254	63.152833
1838.871002	2491.348391	63.157838
1838.447830	2435.537231	63.162842
1837.689638	2387.820639	63.167847
1836.905042	2317.910704	63.172852
1836.173922	2277.709265	63.177857
1835.751948	2223.207761	63.182862
1835.435185	2167.299508	63.187866
1834.342081	2118.840517	63.192871
1834.210872	2062.336225	63.197876
1833.227822	2010.741350	63.202881
1832.577122	1958.201242	63.207886
1831.984005	1897.418086	63.212890
1831.017027	1845.754217	63.217895
1830.486112	1792.127201	63.222900
1829.638416	1742.626677	63.227905
1828.548008	1694.509326	63.232910
1828.319954	1644.797988	63.237914
1827.385624	1610.264789	63.242919
1826.877033	1551.449680	63.247924
1826.127921	1509.981312	63.252929
1825.568007	1461.137060	63.257934
1825.203679	1402.074130	63.262938
1824.342316	1367.734940	63.267943
1823.870151	1301.018759	63.272948
1823.318486	1256.483952	63.277953
1822.508941	1213.936289	63.282958
1821.632775	1149.806630	63.287962
1820.952262	1104.586238	63.292967
1820.322168	1062.592449	63.297972
1819.622292	1019.352981	63.302977
1818.784029	968.107057	63.307982
1818.300533	920.457326	63.312986
1817.492246	879.160223	63.317991
1816.981746	831.382604	63.322996
1816.452620	786.951318	63.328001
1815.500124	733.423535	63.333006
1814.765548	693.043315	63.338010
1814.151363	656.845154	63.343015
1813.314138	610.298144	63.348020
1812.532294	565.056102	63.353025
1812.108091	525.871293	63.358030
1811.554947	491.117814	63.363034
1810.436532	453.322343	63.368039
1810.084001	404.442414	63.373044
1809.183529	366.692989	63.378049
1808.579119	334.381253	63.383054
1807.701595	289.864889	63.388058
1807.195186	255.229134	63.393063
1806.713976	216.620334	63.398068
1805.790482	177.717595	63.403073
1804.909384	141.753915	63.408078
1804.210147	106.378022	63.413082
1803.416365	89.257382	63.418087
1802.796306	44.003900	63.423092
1802.148991	13.309719	63.428097
1801.513919	-17.272802	63.433102
1800.946996	-39.787624	63.438106
1800.152653	-55.408370	63.443111
1799.081843	-84.964380	63.448116
1796.950589	-69.306381	63.453121
1792.248497	27.125128	63.458126
1792.884969	20.785857	63.463130
1793.631025	17.560923	63.468135
1794.318238	12.082473	63.473140
1793.720123	20.705393	63.478145
1793.906623	13.347933	63.483150
1793.203463	-2.938607	63.488154
1791.752700	18.430209	63.493159
1791.178213	16.141918	63.498164
1790.426160	17.991240	63.503169
1789.973456	23.342645	63.508174
1789.432533	17.471024	63.513178
1788.754504	30.301210	63.518183
1788.243418	21.513879	63.523188
1787.258684	23.354420	63.528193
1786.773889	28.218928	63.533198
1786.166875	31.718321	63.538202
1784.868251	39.695572	63.543207
1784.858276	27.805733	63.548212
1784.633434	31.804241	63.553217
1783.278442	38.776492	63.558222
1782.983348	26.723777	63.563226
1782.227461	40.667017	63.568231
1782.001995	39.398754	63.573236
1781.424360	38.832946	63.578241
1779.598011	35.011998	63.583246
1779.472770	41.074635	63.588250
1778.837947	30.171817	63.593255
1778.536726	31.769786	63.598260
1778.037207	33.495436	63.603265
1777.114406	39.848720	63.608270
1776.496770	29.036212	63.613274
1774.819945	39.390001	63.618279
1774.859167	31.925036	63.623284
1774.311985	49.927219	63.628289
1773.310587	41.722352	63.633294
1773.072728	30.029544	63.638298
1771.854186	34.367195	63.643303
1771.422116	40.875936	63.648308
1771.403392	36.025224	63.653313
1770.592507	41.993319	63.658318
1769.902869	35.864622	63.663322
1768.977091	49.916850	63.668327
1768.651057	42.511460	63.673332
1767.921985	38.943616	63.678337
1767.301728	32.786557	63.683342
1766.651234	32.656511	63.688346
1766.070284	45.291528	63.693351
1765.606975	38.849354	63.698356
1765.001762	34.161162	63.703361
1764.012494	46.227105	63.708366
1762.841561	36.368183	63.713370
1762.325636	39.408429	63.718375
1762.196699	37.416808	63.723380
1761.585227	37.881367	63.728385
1760.233050	50.250943	63.733390
1759.832234	39.921227	63.738394
1759.122849	47.007005	63.743399
1758.886503	45.494474	63.748404
1757.788012	35.980432	63.753409
1756.950970	42.531410	63.758414
1756.852772	36.868596	63.763418
1756.007910	43.463392	63.768423
1755.156470	42.625689	63.773428
1754.628921	37.832128	63.778433
1754.012535	43.928608	63.783438
1753.403707	39.198415	63.788442
1752.753857	39.432535	63.793447
1752.344539	38.909387	63.798452
1751.870008	45.188339	63.803457
1750.933837	39.731137	63.808462
1750.682493	20.554905	63.813466
1749.586038	51.571796	63.818471
1748.526196	38.937225	63.823476
1747.824680	38.537750	63.828481
1746.927847	36.926690	63.833486
1747.171542	27.984810	63.838490
1746.136538	42.396570	63.843495
1745.396212	44.870078	63.848500
1744.556454	40.726901	63.853505
1744.118410	37.141232	63.858510
1743.805874	31.750574	63.863514
1742.823701	37.641800	63.868519
1742.331264	33.180125	63.873524
1742.234795	41.075288	63.878529
1741.404816	38.928502	63.883534
1740.251173	41.701032	63.888538
1739.115775	39.842440	63.893543
1738.514074	38.088322	63.898548
1738.351959	35.425478	63.903553
1737.645615	34.336087	63.908558
1737.009735	35.271293	63.913562
1736.342695	43.638682	63.918567
1736.056196	34.255889	63.923572
1735.524440	30.973680	63.928577
1734.494118	34.070391	63.933582
1733.454884	31.411232	63.938586
1732.448733	30.229112	63.943591
1732.465367	33.974814	63.948596
1731.649876	36.692066	63.953601
1730.986946	30.790948	63.958606
1730.639309	35.739336	63.963610
1729.752912	42.102622	63.968615
1729.267553	25.742065	63.973620
1729.247598	37.685608	63.978625
1728.115031	41.618552	63.983630
1726.986303	33.531702	63.988634
1726.520096	41.001474	63.993639
1725.993685	37.134961	63.998644
1725.460533	32.294991	64.003649
1724.527799	41.787912	64.008654
1723.414706	33.674926	64.013658
1722.657587	37.532476	64.018663
1722.809697	33.039402	64.023668
1721.999504	28.435816	64.028673
1720.842133	45.798487	64.033678
1720.160347	38.088497	64.038682
1719.654021	35.522898	64.043687
1719.432885	32.820546	64.048692
1718.768887	34.838826	64.053697
1718.235978	36.511444	64.058702
1717.890996	31.890743	64.063706
1716.490617	38.370352	64.068711
1715.529084	44.974227	64.073716
1714.979271	43.686522	64.078721
1714.194026	41.750254	64.083726
1713.951907	27.967159	64.088730
1713.413328	40.122375	64.093735
1712.749841	35.195878	64.098740
1712.750347	33.541660	64.103745
1711.232124	36.551871	64.108750
1710.559593	33.536446	64.113754
1709.685253	42.330988	64.118759
1709.178362	39.435907	64.123764
1708.665650	38.528654	64.128769
1708.153364	35.112474	64.133774
1707.991484	34.013888	64.138778
1706.481655	41.163725	64.143783
1705.590199	35.533867	64.148788
1705.298556	31.557537	64.153793
1704.402424	35.511283	64.158798
1703.809644	32.273465	64.163802
1703.235825	42.570378	64.168807
1702.927395	43.527700	64.173812
1702.846360	33.049448	64.178817
1701.961633	37.146459	64.183822
1700.575072	31.631509	64.188826
1699.904378	37.094820	64.193831
1699.296282	34.099125	64.198836
1699.147933	34.884370	64.203841
1698.629219	39.397900	64.208846
1698.054374	33.258880	64.213850
1696.962202	40.373925	64.218855
1695.960984	30.871278	64.223860
1695.309070	35.879034	64.228865
1694.935027	38.090957	64.233870
1694.430007	31.199703	64.238874
1693.137723	38.928411	64.243879
1692.566142	47.141879	64.248884
1692.053252	40.381178	64.253889
1691.126020	33.172218	64.258894
1690.927968	30.358974	64.263898
1690.296931	31.112077	64.268903
1689.728927	43.243587	64.273908
1689.542681	41.809836	64.278913
1688.566778	26.966922	64.283918
1687.778994	35.315646	64.288922
1686.654945	53.567149	64.293927
1686.774752	35.199266	64.298932
1685.798983	38.823479	64.303937
1684.494636	46.308113	64.308942
1684.076656	41.191245	64.313946
1683.454152	22.226943	64.318951
1682.761140	42.988210	64.323956
1682.719761	30.231341	64.328961
1681.870428	52.349936	64.333966
1681.525075	29.788832	64.338970
1680.190700	34.985410	64.343975
1679.332636	33.073336	64.348980
1679.162220	30.667275	64.353985
1678.541027	33.981289	64.358990
1678.209775	30.454365	64.363994
1676.934260	32.883588	64.368999
1676.276812	32.738899	64.374004
1675.627813	35.953256	64.379009
1675.027317	41.484268	64.384014
1674.843228	41.161895	64.389018
1674.007020	48.434986	64.394023
1672.719673	41.511881	64.399028
1671.845986	39.110295	64.404033
1671.033060	43.443487	64.409038
1670.924253	38.417860	64.414042
1670.379828	37.309077	64.419047
1669.707769	35.116733	64.424052
1669.561942	40.206533	64.429057
1669.154396	34.260138	64.434062
1668.275259	41.391816	64.439066
1667.057979	53.888233	64.444071
1666.698604	45.794318	64.449076
1666.188762	33.318434	64.454081
1665.120773	35.853468	64.459086
1664.097043	29.741606	64.464090
1663.213068	42.388493	64.469095
1662.982147	41.598911	64.474100
1662.649967	38.292901	64.479105
1662.307651	34.811889	64.484110
1661.899883	30.477130	64.489114
1660.575637	33.655247	64.494119
1659.502176	26.529454	64.499124
1659.137085	29.611986	64.504129
1658.648436	39.116382	64.509134
1658.261165	31.698670	64.514138
1657.325030	37.696147	64.519143
1656.647076	34.591715	64.524148
1656.167102	27.239193	64.529153
1655.428466	40.913213	64.534158
1655.165159	33.923651	64.539162
1653.505498	31.635881	64.544167
1652.855434	35.380251	64.549172
1652.618346	45.823952	64.554177
1651.648532	34.572276	64.559182
1651.656333	21.244653	64.564186
1651.103693	30.212023	64.569191
1650.367089	29.045465	64.574196
1649.357762	33.578586	64.579201
1648.111981	30.490239	64.584206
1648.152509	33.424767	64.589210
1647.593653	44.998181	64.594215
1646.832738	38.451927	64.599220
1645.953533	30.989362	64.604225
1645.295561	30.616113	64.609230
1644.541659	32.098351	64.614234
1644.168285	26.668492	64.619239
1643.896449	23.936358	64.624244
1643.189491	35.679943	64.629249
1641.887701	34.298823	64.634254
1641.581526	28.315834	64.639258
1640.681858	23.955143	64.644263
1640.481107	42.113593	64.649268
1639.617347	22.490641	64.654273
1638.428054	32.711862	64.659278
1638.237271	34.530415	64.664282
1637.787311	32.733296	64.669287
1637.058269	27.047709	64.674292
1636.150811	27.701236	64.679297
1635.032284	31.373371	64.684302
1634.601930	32.807370	64.689306
1633.872659	38.054502	64.694311
1633.524877	29.919340	64.699316
1633.894161	29.170032	64.704321
1632.160758	27.810172	64.709326
1631.682061	24.240449	64.714330
1631.106365	39.686258	64.719335
1630.445504	29.509854	64.724340
1629.422721	24.213120	64.729345
1628.422958	45.540345	64.734350
1628.018873	38.260923	64.739354
1627.585679	31.607428	64.744359
1627.290987	38.089627	64.749364
1626.990523	34.682395	64.754369
1625.382445	23.689822	64.759374
1624.785704	38.142370	64.764378
1624.235793	39.406135	64.769383
1623.666502	32.771106	64.774388
1623.403593	29.618099	64.779393
1621.958758	35.317938	64.784398
1621.478457	21.187944	64.789402
1620.840104	26.666629	64.794407
1620.124035	32.514042	64.799412
1620.185053	34.202712	64.804417
1618.843017	34.499516	64.809422
1618.354195	32.055736	64.814426
1617.596314	30.469957	64.819431
1617.000892	25.583141	64.824436
1616.703251	24.764741	64.829441
1615.500975	36.320518	64.834446
1614.741302	31.883981	64.839450
1614.321938	32.907818	64.844455
1613.421409	27.012946	64.849460
1613.459879	32.428269	64.854465
1612.659405	32.071359	64.859470
1611.673277	18.012264	64.864474
1610.986991	30.353366	64.869479
1610.585779	20.039536	64.874484
1610.110916	16.361981	64.879489
1609.343065	34.298280	64.884494
1608.572602	23.904340	64.889498
1607.696587	29.985315	64.894503
1607.149347	29.167145	64.899508
1606.797776	33.706172	64.904513
1605.740769	37.676044	64.909518
1604.871811	27.501170	64.914522
1604.086625	33.862600	64.919527
1603.783091	20.280101	64.924532
1603.327939	22.170614	64.929537
1602.938118	33.756593	64.934542
1601.917650	38.919109	64.939546
1601.350429	36.738514	64.944551
1600.746889	32.458522	64.949556
1600.280694	24.392643	64.954561
1598.793058	37.550164	64.959566
1598.512515	20.821242	64.964570
1597.831395	39.092265	64.969575
1597.623275	34.970222	64.974580
1596.543307	28.501484	64.979585
1595.029660	39.524860	64.984590
1594.937962	29.160280	64.989594
1594.656078	36.831008	64.994599
1594.048357	31.476233	64.999604
1593.925924	36.011975	65.004609
1592.924782	38.072806	65.009614
1591.960525	35.799176	65.014618
1591.119211	39.137140	65.019623
1590.839863	39.870664	65.024628
1590.304594	25.982790	65.029633
1589.075960	31.865910	65.034638
1588.635297	32.987749	65.039642
1587.807167	34.387181	65.044647
1587.401662	26.955039	65.049652
1587.090491	28.103613	65.054657
1585.770812	24.191281	65.059662
1585.191462	23.723559	65.064666
1584.611686	32.595904	65.069671
1584.251966	30.317695	65.074676
1583.858543	25.707870	65.079681
1582.461074	34.768469	65.084686
1582.061625	20.046921	65.089690
1581.575915	26.743962	65.094695
1580.949460	33.717248	65.099700
1579.606689	28.868751	65.104705
1578.913487	31.432581	65.109710
1578.595691	29.609745	65.114714
1577.959452	30.316394	65.119719
1577.862585	31.528691	65.124724
1577.455614	27.602242	65.129729
1576.324035	32.512767	65.134734
1575.679188	27.031437	65.139738
1575.004690	36.056025	65.144743
1573.917451	36.523676	65.149748
1573.168012	33.067938	65.154753
1572.442943	34.914611	65.159758
1572.377251	26.770917	65.164762
1571.899221	26.227178	65.169767
1570.564466	25.507324	65.174772
1569.871443	22.280739	65.179777
1569.396017	32.705525	65.184782
1569.196351	24.532657	65.189786
1568.829531	33.692859	65.194791
1567.481169	29.420828	65.199796
1566.983151	33.732397	65.204801
1566.167367	33.382665	65.209806
1565.834046	27.809268	65.214810
1564.649115	26.780194	65.219815
1563.747784	25.691871	65.224820
1563.513388	27.312359	65.229825
1563.033545	32.666529	65.234830
1562.658510	28.224091	65.239834
1561.762308	29.937111	65.244839
1560.838307	32.182811	65.249844
1560.615345	25.178976	65.254849
1559.613592	28.528246	65.259854
1559.347051	27.957216	65.264858
1558.115723	39.574399	65.269863
1557.257072	34.101811	65.274868
1557.223773	17.861886	65.279873
1556.587995	34.159305	65.284878
1555.538851	31.135955	65.289882
1554.450600	34.607777	65.294887
1554.199089	28.661849	65.299892
1553.942410	18.131114	65.304897
1553.142822	28.743015	65.309902
1552.517650	27.136172	65.314906
1551.743077	25.310223	65.319911
1551.304651	30.672005	65.324916
1550.966341	35.194738	65.329921
1549.794723	24.738406	65.334926
1548.844933	32.035873	65.339930
1548.423877	24.749711	65.344935
1548.013383	33.122094	65.349940
1547.229066	29.958903	65.354945
1545.791841	34.009706	65.359950
1545.696453	28.668159	65.364954
1545.374125	30.722076	65.369959
1544.578926	35.998625	65.374964
1543.703739	25.911500	65.379969
1542.691703	35.092220	65.384974
1542.330826	32.249671	65.389978
1542.230425	24.575105	65.394983
1541.413266	29.631221	65.399988
1540.607693	28.314810	65.404993
1539.507340	34.160222	65.409998
1539.327965	33.794534	65.415002
1538.720638	33.176731	65.420007
1537.751250	21.865132	65.425012
1536.958078	26.619403	65.430017
1536.395758	34.173845	65.435022
1536.159868	32.541422	65.440026
1535.373081	43.152880	65.445031
1534.185909	35.980558	65.450036
1533.938691	19.861355	65.455041
1533.222347	44.177519	65.460046
1533.214400	25.538245	65.465050
1531.885762	44.662768	65.470055
1531.084125	32.499789	65.475060
1530.879387	28.372488	65.480065
1529.327876	37.631047	65.485070
1529.127855	29.462969	65.490074
1528.342374	31.328713	65.495079
1527.714372	35.419676	65.500084
1527.629266	28.173175	65.505089
1526.917440	30.175445	65.510094
1526.112634	27.822891	65.515098
1525.055403	36.157695	65.520103
1524.348881	30.142148	65.525108
1524.348767	33.154088	65.530113
1523.519209	39.155170	65.535118
1522.566614	30.491680	65.540122
1522.116214	28.065469	65.545127
1521.301487	39.545509	65.550132
1520.998946	20.394829	65.555137
1519.597497	25.884401	65.560142
1519.092513	18.666776	65.565146
1518.749066	31.710328	65.570151
1518.288806	29.968483	65.575156
1517.715821	20.279618	65.580161
1516.315955	40.799978	65.585166
1516.066545	28.672262	65.590170
1515.532755	32.226302	65.595175
1515.096978	26.297046	65.600180
1514.052428	25.474341	65.605185
1512.918306	26.326347	65.610190
1512.673749	32.302281	65.615194
1512.340140	26.118679	65.620199
1511.486050	29.059738	65.625204
1510.799864	23.367386	65.630209
1509.782265	30.786022	65.635214
1509.685308	26.619520	65.640218
1509.109311	14.102180	65.645223
1507.755622	20.640690	65.650228
1507.454720	30.701867	65.655233
1506.639134	33.062817	65.660238
1506.553552	24.077073	65.665242
1505.273148	33.800325	65.670247
1504.240402	30.099478	65.675252
1503.991957	25.231674	65.680257
1503.212031	28.824826	65.685262
1502.852795	27.374428	65.690266
1502.347278	26.641111	65.695271
1501.801037	27.418630	65.700276
1501.081839	34.583279	65.705281
1500.090516	35.187103	65.710286
1499.336409	25.755673	65.715290
1499.449723	28.798471	65.720295
1498.175338	34.466555	65.725300
1497.130500	26.205654	65.730305
1496.586554	37.809822	65.735310
1496.485700	24.048490	65.740314
1496.007010	32.966282	65.745319
1494.574270	38.467150	65.750324
1494.165704	18.713606	65.755329
1493.634890	27.191838	65.760334
1493.201230	23.124573	65.765338
1492.060357	27.016350	65.770343
1491.307521	30.617817	65.775348
1491.213074	25.771274	65.780353
1490.714030	22.739385	65.785358
1489.888414	19.347821	65.790362
1488.982280	23.167605	65.795367
1488.032708	31.379657	65.800372
1488.096299	26.599461	65.805377
1486.865201	25.785911	65.810382
1486.018886	24.627375	65.815386
1485.369592	29.002416	65.820391
1485.146126	35.358188	65.825396
1484.803148	26.719266	65.830401
1483.688449	32.630054	65.835406
1482.933686	30.532905	65.840410
1482.688593	25.609380	65.845415
1481.816586	28.669986	65.850420
1481.100365	27.757274	65.855425
1480.282207	28.664737	65.860430
1479.760833	25.401441	65.865434
1479.401622	22.763636	65.870439
1478.170449	20.939309	65.875444
1477.565922	24.548748	65.880449
1476.770432	24.027091	65.885454
1476.622029	23.389989	65.890458
1476.037901	28.986237	65.895463
1475.131264	26.258811	65.900468
1474.532230	29.630844	65.905473
1473.892472	31.426139	65.910478
1473.228109	17.768558	65.915482
1472.156190	27.248960	65.920487
1471.292255	23.142846	65.925492
1470.880079	17.031664	65.930497
1470.197611	31.448955	65.935502
1470.364252	29.348885	65.940506
1469.315947	20.456216	65.945511
1468.380407	24.361101	65.950516
1468.083361	21.262426	65.955521
1467.305248	35.441040	65.960526
1466.561880	34.204650	65.965530
1465.693134	26.895038	65.970535
1464.960064	22.477981	65.975540
1465.008442	21.498959	65.980545
1464.197388	37.221865	65.985550
1463.383029	25.079868	65.990554
1462.686112	28.563648	65.995559
1461.928432	33.540951	66.000564
1461.257056	23.771547	66.005569
1460.145155	23.246564	66.010574
1459.430397	28.351081	66.015578
1459.415913	30.179472	66.020583
1458.800763	35.739655	66.025588
1458.479332	28.054494	66.030593
1457.290222	27.917084	66.035598
1456.789135	33.129568	66.040602
1456.383012	33.422797	66.045607
1455.120692	33.192947	66.050612
1454.586412	26.673828	66.055617
1453.914261	33.643359	66.060622
1453.482210	19.882635	66.065626
1452.634909	31.072978	66.070631
1451.390009	37.999496	66.075636
1451.387779	29.946650	66.080641
1450.681862	28.548201	66.085646
1450.595405	29.627963	66.090650
1449.615785	27.312679	66.095655
1448.353410	25.398711	66.100660
1448.247976	28.559845	66.105665
1447.575689	28.337151	66.110670
1446.965825	30.930344	66.115674
1446.406369	30.968831	66.120679
1445.177337	33.786576	66.125684
1444.943742	28.913266	66.130689
1443.539567	32.868986	66.135694
1443.011725	40.856343	66.140698
1442.559190	32.752062	66.145703
1442.240798	38.507930	66.150708
1441.625409	29.658428	66.155713
1440.410238	34.489253	66.160718
1440.058952	30.544520	66.165722
1439.642807	31.208338	66.170727
1439.035900	40.539166	66.175732
1438.475213	25.122638	66.180737
1437.185235	37.892436	66.185742
1436.832626	34.725325	66.190746
1436.466825	37.899456	66.195751
1435.374333	36.800560	66.200756
1434.688704	25.253108	66.205761
1434.170425	29.345573	66.210766
1433.591686	23.945243	66.215770
1433.146619	35.585737	66.220775
1431.986981	28.957859	66.225780
1431.614011	23.786593	66.230785
1430.794626	35.057659	66.235790
1430.328037	19.156270	66.240794
1429.248154	24.456011	66.245799
1428.546120	30.369040	66.250804
1427.922005	30.491921	66.255809
1427.211854	25.144016	66.260814
1427.077783	33.264324	66.265818
1426.854388	21.045770	66.270823
1425.827808	24.392724	66.275828
1425.285560	30.119515	66.280833
1424.633263	31.409052	66.285838
1423.500057	30.737665	66.290842
1423.189398	38.487085	66.295847
1422.366080	27.261131	66.300852
1421.300237	29.366999	66.305857
1420.516740	26.667331	66.310862
1420.131305	31.746325	66.315866
1419.753915	35.180910	66.320871
1418.925661	35.806155	66.325876
1418.774267	25.531514	66.330881
1417.844100	28.632921	66.335886
1417.430831	23.799211	66.340890
1416.747674	27.249277	66.345895
1415.507863	33.153167	66.350900
1414.938554	24.745770	66.355905
1414.498211	29.317843	66.360910
1413.922869	27.578541	66.365914
1412.953912	36.787145	66.370919
1412.261168	25.647674	66.375924
1412.122982	24.520114	66.380929
1411.068279	26.610023	66.385934
1410.270349	37.183849	66.390938
1409.685148	26.840966	66.395943
1409.290751	26.320235	66.400948
1408.649078	32.710937	66.405953
1407.347288	32.168850	66.410958
1406.733521	39.081805	66.415962
1406.342782	22.487144	66.420967
1406.037661	29.346308	66.425972
1405.448656	30.996362	66.430977
1404.171633	32.041433	66.435982
1403.838136	31.048991	66.440986
1403.394805	38.962997	66.445991
1402.284857	36.800904	66.450996
1401.607435	35.394785	66.456001
1400.678489	34.959016	66.461006
1400.619610	27.787206	66.466010
1400.484727	32.214542	66.471015
1399.124890	45.944758	66.476020
1398.209345	27.091808	66.481025
1397.532844	32.381064	66.486030
1397.430312	31.202107	66.491034
1397.077760	36.163919	66.496039
1395.782271	41.740790	66.501044
1395.445102	28.360798	66.506049
1394.510297	28.184574	66.511054
1393.659457	34.116533	66.516058
1393.092492	30.975616	66.521063
1392.477974	39.741551	66.526068
1391.916777	22.909068	66.531073
1391.488310	36.880738	66.536078
1390.762482	25.808033	66.541082
1389.950684	29.045171	66.546087
1389.370958	35.962178	66.551092
1388.970702	26.424087	66.556097
1387.506385	38.032631	66.561102
1387.107254	32.378266	66.566106
1386.930164	36.290357	66.571111
1386.100178	39.216586	66.576116
1385.110137	21.760011	66.581121
1384.113435	36.728717	66.586126
1383.811162	28.182692	66.591130
1383.350194	28.812644	66.596135
1383.281101	26.587619	66.601140
1382.530394	32.194592	66.606145
1381.505367	34.924749	66.611150
1380.933096	23.778758	66.616154
1379.791111	23.930350	66.621159
1378.955565	33.485174	66.626164
1378.803576	27.901913	66.631169
1378.045780	26.924879	66.636174
1377.963332	30.680005	66.641178
1376.610533	21.058369	66.646183
1375.712292	32.015559	66.651188
1375.474430	28.207346	66.656193
1374.926221	26.522085	66.661198
1373.993833	30.953186	66.666202
1373.495257	21.034930	66.671207
1372.529628	34.927982	66.676212
1372.363572	32.688409	66.681217
1371.227876	28.376378	66.686222
1370.406720	23.646936	66.691226
1370.285626	30.784346	66.696231
1369.644502	32.277118	66.701236
1369.155726	26.132400	66.706241
1368.300545	37.636244	66.711246
1367.496272	29.671471	66.716250
1367.523421	30.430412	66.721255
1366.077082	28.780685	66.726260
1365.543326	26.331487	66.731265
1365.018516	31.410564	66.736270
1363.880938	35.002259	66.741274
1363.482494	22.832043	66.746279
1362.725194	29.291593	66.751284
1362.295263	27.636418	66.756289
1361.552211	29.875498	66.761294
1360.776137	25.741268	66.766298
1359.939784	23.672897	66.771303
1359.291202	36.537881	66.776308
1359.069346	22.778465	66.781313
1358.362893	27.244616	66.786318
1357.677040	25.300552	66.791322
1357.237429	30.897501	66.796327
1356.680316	26.075630	66.801332
1355.293460	35.517829	66.806337
1354.415047	35.236465	66.811342
1353.880256	28.845184	66.816346
1354.205983	22.921071	66.821351
1353.078653	29.716977	66.826356
1352.188676	20.322975	66.831361
1351.439767	28.419590	66.836366
1351.143942	29.431714	66.841370
1350.785966	32.869528	66.846375
1349.336033	35.690894	66.851380
1348.989593	28.476493	66.856385
1348.313649	28.945089	66.861390
1347.876945	33.281636	66.866394
1346.965659	28.951291	66.871399
1346.129851	36.722692	66.876404
1346.334171	21.941510	66.881409
1345.006594	35.322844	66.886414
1343.771629	29.274671	66.891418
1343.370966	37.292282	66.896423
1343.068856	26.158548	66.901428
1343.176798	16.689497	66.906433
1341.890060	37.663416	66.911438
1340.916043	28.024162	66.916442
1340.547844	24.676628	66.921447
1339.817666	28.042726	66.926452
1338.866300	20.676920	66.931457
1338.428563	21.664297	66.936462
1337.755835	19.819074	66.941466
1337.354131	20.141579	66.946471
1336.178152	30.195212	66.951476
1335.632505	19.905994	66.956481
1335.045831	28.396278	66.961486
1334.725333	26.556562	66.966490
1334.085563	29.345337	66.971495
1332.950988	28.152255	66.976500
1332.279126	18.215829	66.981505
1332.087979	18.738244	66.986510
1331.501861	25.167433	66.991514
1330.338475	24.273812	66.996519
1329.655632	29.756471	67.001524
1329.551475	27.398256	67.006529
1328.217304	26.840857	67.011534
1327.840024	25.528968	67.016538
1327.133492	17.338952	67.021543
1326.435308	25.635658	67.026548
1326.121288	8.434354	67.031553
1325.277747	26.873118	67.036558
1324.806817	23.057810	67.041562
1324.293479	14.086482	67.046567
1323.241359	34.348192	67.051572
1322.237645	20.944884	67.056577
1321.741870	23.182508	67.061582
1321.169112	29.887111	67.066586
1321.056555	24.772236	67.071591
1319.748512	25.036983	67.076596
1319.186125	26.575594	67.081601
1318.713959	24.047233	67.086606
1318.162035	15.316998	67.091610
1317.170315	16.643172	67.096615
1316.353509	15.107856	67.101620
1316.148871	22.469846	67.106625
1315.814753	23.360332	67.111630
1314.508736	32.404932	67.116634
1314.117337	19.076170	67.121639
1313.250810	27.211990	67.126644
1312.787263	27.146952	67.131649
1311.475568	23.146774	67.136654
1311.025913	24.971806	67.141658
1310.509985	24.341105	67.146663
1310.130705	30.470922	67.151668
1310.252744	17.577760	67.156673
1309.118449	34.228827	67.161678
1308.059413	29.199767	67.166682
1307.299069	21.516611	67.171687
1306.427387	22.035258	67.176692
1306.058199	23.424889	67.181697
1305.575731	27.278300	67.186702
1305.045558	29.051481	67.191706
1304.203453	20.719027	67.196711
1303.312953	26.231549	67.201716
1303.039556	16.345325	67.206721
1301.710237	24.936330	67.211726
1301.004000	26.418969	67.216730
1300.592880	19.482939	67.221735
1299.812388	26.280490	67.226740
1299.492799	25.665884	67.231745
1299.322152	26.178736	67.236750
1298.104895	28.002805	67.241754
1297.503216	22.907349	67.246759
1297.140437	22.058345	67.251764
1296.175357	16.710016	67.256769
1295.305767	16.023584	67.261774
1294.997187	26.628433	67.266778
1294.497020	24.516099	67.271783
1293.480060	25.305420	67.276788
1292.604737	14.742215	67.281793
1292.159548	25.384550	67.286798
1291.567260	25.306869	67.291802
1291.174252	23.191692	67.296807
1289.986791	32.646370	67.301812
1289.733010	13.527446	67.306817
1289.094922	20.278704	67.311822
1288.366707	16.743999	67.316826
1287.317423	17.008623	67.321831
1286.406640	26.154392	67.326836
1286.464497	15.058065	67.331841
1285.883255	28.022725	67.336846
1285.027159	25.577487	67.341850
1284.282877	16.057857	67.346855
1283.564241	20.352502	67.351860
1283.416276	18.747128	67.356865
1282.512953	33.358820	67.361870
1281.927967	27.237306	67.366874
1281.148375	19.199266	67.371879
1279.984684	26.844617	67.376884
1279.487419	19.177992	67.381889
1278.930478	22.008801	67.386894
1278.485962	27.978685	67.391898
1277.614009	19.270957	67.396903
1276.387796	28.758606	67.401908
1276.477127	20.773222	67.406913
1276.178901	23.807318	67.411918
1275.039310	23.501276	67.416922
1274.404329	14.495688	67.421927
1273.455086	19.468796	67.426932
1273.393072	19.614306	67.431937
1272.218136	25.190981	67.436942
1271.401619	28.577131	67.441946
1271.035827	23.105146	67.446951
1270.156732	27.767493	67.451956
1270.159685	18.692016	67.456961
1269.301457	23.343161	67.461966
1268.234963	29.459243	67.466970
1268.247489	16.411617	67.471975
1266.848763	24.734561	67.476980
1266.277639	20.632433	67.481985
1265.818869	18.526140	67.486990
1265.396239	22.994492	67.491994
1264.615863	10.091861	67.496999
1263.541390	23.395127	67.502004
1262.982541	18.682366	67.507009
1262.198175	22.996928	67.512014
1261.977307	20.996308	67.517018
1261.253444	17.279576	67.522023
1260.468046	28.748687	67.527028
1260.095999	18.548583	67.532033
1259.639980	18.499704	67.537038
1258.553196	11.488195	67.542042
1258.076431	19.959433	67.547047
1256.999722	26.196986	67.552052
1256.005489	18.368119	67.557057
1255.337662	22.096471	67.562062
1254.627724	11.581104	67.567066
1254.422211	10.492644	67.572071
1253.660447	13.466404	67.577076
1253.815313	15.189019	67.582081
1253.121428	13.813946	67.587086
1252.216332	20.878891	67.592090
1251.753420	15.206319	67.597095
1250.174377	25.055993	67.602100
1249.804996	17.673385	67.607105
1249.350310	23.709540	67.612110
1248.834761	17.278966	67.617114
1247.989623	20.879398	67.622119
1246.909458	26.278595	67.627124
1246.462352	17.746173	67.632129
1246.130840	12.467435	67.637134
1245.420128	25.496836	67.642138
1244.752129	22.129181	67.647143
1243.927804	29.539245	67.652148
1243.914540	22.737079	67.657153
1242.776942	19.816240	67.662158
1241.971308	21.841382	67.667162
1241.279958	21.052514	67.672167
1240.816348	33.837636	67.677172
1240.069908	21.139337	67.682177
1239.545573	24.359193	67.687182
1238.822510	24.564083	67.692186
1237.531724	18.442850	67.697191
1236.803020	19.779272	67.702196
1236.309920	13.472862	67.707201
1236.138435	17.852399	67.712206
1235.712381	24.549454	67.717210
1235.531194	20.711750	67.722215
1234.184556	33.610471	67.727220
1233.651628	25.107463	67.732225
1233.037095	28.767425	67.737230
1231.866133	22.649217	67.742234
1231.426583	29.994949	67.747239
1230.642355	20.746608	67.752244
1230.335133	24.554817	67.757249
1229.102835	24.077463	67.762254
1228.183976	28.077542	67.767258
1228.010495	18.774666	67.772263
1227.570028	16.380052	67.777268
1227.248051	23.973582	67.782273
1226.035838	27.170359	67.787278
1225.505623	30.708110	67.792282
1225.285955	15.212222	67.797287
1224.304129	28.570155	67.802292
1223.429127	17.573282	67.807297
1222.983462	20.599287	67.812302
1222.128564	22.506116	67.817306
1221.614079	17.716929	67.822311
1220.616718	25.545581	67.827316
1220.160937	22.237226	67.832321
1219.899836	19.987551	67.837326
1219.052560	22.142318	67.842330
1218.506637	18.554995	67.847335
1217.625525	36.070967	67.852340
1217.009954	16.639020	67.857345
1216.049223	19.798965	67.862350
1215.514324	21.822063	67.867354
1215.115533	17.033404	67.872359
1214.496449	24.617410	67.877364
1213.411447	21.021194	67.882369
1212.928352	15.165768	67.887374
1212.363899	15.540979	67.892378
1211.772437	8.539038	67.897383
1210.480215	19.224603	67.902388
1210.128180	9.876015	67.907393
1209.506663	11.890810	67.912398
1209.298016	26.180741	67.917402
1208.629326	12.981262	67.922407
1207.423931	20.338389	67.927412
1206.832173	20.629637	67.932417
1206.662737	16.384807	67.937422
1205.856306	20.557817	67.942426
1204.746237	15.415504	67.947431
1204.227841	23.461299	67.952436
1204.006063	13.074899	67.957441
1203.186556	18.506774	67.962446
1202.113286	18.943975	67.967450
1201.699345	15.494936	67.972455
1201.330357	15.768107	67.977460
1200.484770	11.820026	67.982465
1199.605147	15.487454	67.987470
1199.011372	15.790063	67.992474
1198.787709	16.320812	67.997479
1197.364883	26.929389	68.002484
1197.311870	24.015867	68.007489
1197.213246	23.336177	68.012494
1195.646984	22.194458	68.017498
1194.876888	19.089050	68.022503
1194.324354	25.665879	68.027508
1193.876940	35.819743	68.032513
1193.345546	21.516678	68.037518
1192.293187	17.631441	68.042522
1192.143408	9.017065	68.047527
1191.206087	20.313229	68.052532
1190.351221	16.898040	68.057537
1189.343684	30.578605	68.062542
1188.993564	16.554214	68.067546
1188.657495	14.057855	68.072551
1188.301109	29.344226	68.077556
1187.314490	13.829967	68.082561
1186.223502	23.345026	68.087566
1185.662598	21.605061	68.092570
1185.434173	14.524895	68.097575
1184.056996	21.806851	68.102580
1183.571606	19.586541	68.107585
1183.551795	19.001546	68.112590
1182.803712	12.983271	68.117594
1181.985391	9.999076	68.122599
1181.261157	22.343106	68.127604
1180.841898	17.142986	68.132609
1180.127294	22.334267	68.137614
1178.835200	25.225235	68.142618
1178.599716	21.429287	68.147623
1177.806749	21.547543	68.152628
1177.661458	19.159612	68.157633
1176.538707	18.100334	68.162638
1175.588878	23.743748	68.167642
1175.340615	22.602171	68.172647
1174.918304	28.243695	68.177652
1174.099422	19.989602	68.182657
1173.200350	21.805704	68.187662
1172.629458	20.422132	68.192666
1172.490577	18.854745	68.197671
1171.370457	31.827848	68.202676
1171.005551	21.705475	68.207681
1170.225590	21.375404	68.212686
1169.126095	10.554606	68.217690
1168.833442	12.304230	68.222695
1167.694494	21.658193	68.227700
1167.582083	13.422638	68.232705
1166.469569	14.930499	68.237710
1165.518625	25.462468	68.242714
1165.342089	32.674920	68.247719
1164.633943	27.583817	68.252724
1164.711873	15.721092	68.257729
1163.259433	17.875926	68.262734
1162.752749	25.744829	68.267738
1162.318348	16.335233	68.272743
1161.661810	19.120403	68.277748
1160.699459	14.178539	68.282753
1160.088845	24.773075	68.287758
1159.425355	22.013411	68.292762
1159.020577	3.640773	68.297767
1157.934179	19.538374	68.302772
1157.380336	14.085284	68.307777
1157.063784	5.658282	68.312782
1156.365755	19.969263	68.317786
1155.741651	25.032622	68.322791
1155.062231	26.634031	68.327796
1154.328294	20.466863	68.332801
1153.318463	8.926943	68.337806
1152.830059	17.628689	68.342810
1152.249528	17.979663	68.347815
1151.476287	33.007492	68.352820
1150.284879	8.788249	68.357825
1149.718661	20.274552	68.362830
1149.126942	32.643251	68.367834
1149.238125	0.717144	68.372839
1148.661369	31.889499	68.377844
1148.014185	8.222349	68.382849
1146.878720	30.509458	68.387854
1146.479047	29.216928	68.392858
1145.645433	13.213176	68.397863
1144.388510	35.104887	68.402868
1143.816825	32.628658	68.407873
1143.693086	12.497231	68.412878
1143.205836	28.786818	68.417882
1142.524815	26.097752	68.422887
1141.492564	26.998370	68.427892
1141.133127	18.616030	68.432897
1140.516620	22.796698	68.437902
1139.326563	20.814620	68.442906
1139.156101	16.396502	68.447911
1138.321681	32.009628	68.452916
1137.869701	14.074984	68.457921
1136.807521	33.761185	68.462926
1136.084698	20.805295	68.467930
1135.791253	15.197259	68.472935
1134.895617	17.138978	68.477940
1134.139617	23.521102	68.482945
1133.799304	30.754869	68.487950
1133.293173	31.761041	68.492954
1132.928199	22.517020	68.497959
1131.642673	17.366379	68.502964
1130.922184	6.485326	68.507969
1130.697717	12.117459	68.512974
1129.219445	22.392695	68.517978
1128.828755	5.093268	68.522983
1128.068658	25.778472	68.527988
1127.667376	21.438064	68.532993
1127.291883	17.634431	68.537998
1126.579865	16.233894	68.543002
1125.892685	12.482989	68.548007
1125.264928	16.484105	68.553012
1124.517717	15.199549	68.558017
1123.826848	19.527659	68.563022
1122.915870	18.221843	68.568026
1122.905296	16.033256	68.573031
1121.794476	21.711752	68.578036
1120.692657	29.238518	68.583041
1120.321024	9.094493	68.588046
1119.621124	15.380964	68.593050
1119.650983	11.339404	68.598055
1118.268010	2.408693	68.603060
1117.581716	15.323836	68.608065
1117.296850	21.531684	68.613070
1116.794483	20.640256	68.618074
1116.255836	-0.776551	68.623079
1115.326969	19.528649	68.628084
1114.891075	18.181965	68.633089
1113.848114	10.252115	68.638094
1113.050867	15.566936	68.643098
1113.134173	10.372051	68.648103
1112.015907	15.693778	68.653108
1111.005664	19.489238	68.658113
1110.670591	17.011655	68.663118
1110.004287	25.066795	68.668122
1109.386636	14.484767	68.673127
1108.092948	11.517861	68.678132
1107.487958	12.085615	68.683137
1107.225965	18.941082	68.688142
1107.010657	20.035038	68.693146
1106.374009	15.361502	68.698151
1105.273085	24.193796	68.703156
1104.879651	20.440327	68.708161
1104.080101	15.709126	68.713166
1102.920297	6.733465	68.718170
1102.861703	10.476905	68.723175
1102.081583	29.539523	68.728180
1101.695564	22.609008	68.733185
1100.460934	19.372523	68.738190
1099.706729	19.609213	68.743194
1099.065018	17.708664	68.748199
1098.692193	27.924778	68.753204
1097.726384	17.756085	68.758209
1097.133444	17.460942	68.763214
1096.464204	18.308567	68.768218
1096.425771	18.734172	68.773223
1095.596814	32.648121	68.778228
1094.613278	19.672220	68.783233
1094.272077	16.640548	68.788238
1093.399696	14.076550	68.793242
1092.792734	30.106070	68.798247
1091.676114	15.243300	68.803252
1091.155978	4.292552	68.808257
1091.179933	14.757770	68.813262
1090.249461	8.051055	68.818266
1089.616207	26.814355	68.823271
1089.115798	24.967023	68.828276
1088.247065	16.306174	68.833281
1086.938701	25.978841	68.838286
1086.246144	31.295944	68.843290
1086.111322	7.626175	68.848295
1085.541760	37.568991	68.853300
1084.893082	12.296825	68.858305
1084.163084	13.726530	68.863310
1083.474620	16.575141	68.868314
1083.312145	20.579525	68.873319
1082.325557	18.549341	68.878324
1081.349409	25.460063	68.883329
1080.991604	17.940039	68.888334
1080.275593	14.912797	68.893338
1079.638559	21.531465	68.898343
1078.592730	20.214001	68.903348
1078.001262	25.857211	68.908353
1077.853515	18.073548	68.913358
1076.886634	16.559030	68.918362
1076.032763	18.905694	68.923367
1075.358105	25.643886	68.928372
1075.333872	23.123171	68.933377
1074.433913	22.313918	68.938382
1073.598750	17.992078	68.943386
1072.876675	17.406834	68.948391
1072.516677	37.988993	68.953396
1071.753717	0.378486	68.958401
1071.097816	23.888675	68.963406
1070.535637	27.888835	68.968410
1069.475098	10.609245	68.973415
1068.311544	12.711870	68.978420
1067.643932	31.720330	68.983425
1067.724912	2.170699	68.988430
1067.369077	39.973442	68.993434
1067.097496	4.558647	68.998439
1065.821094	23.020564	69.003444
1065.213613	18.985773	69.008449
1064.330559	12.460752	69.013454
1063.006740	27.956200	69.018458
1063.086139	14.409129	69.023463
1062.404569	19.344455	69.028468
1061.873210	41.653769	69.033473
1061.312216	19.171376	69.038478
1060.207558	13.794894	69.043482
1059.935264	17.217528	69.048487
1058.747076	32.640946	69.053492
1057.872386	9.177183	69.058497
1057.756491	19.972141	69.063502
1056.854171	13.639415	69.068506
1056.862924	27.330225	69.073511
1056.255918	22.018075	69.078516
1055.221158	16.572131	69.083521
1054.898273	24.908529	69.088526
1053.659927	24.850099	69.093530
1053.059981	17.523136	69.098535
1052.279136	23.880847	69.103540
1052.038733	17.974238	69.108545
1051.117027	23.133841	69.113550
1050.357641	24.210277	69.118554
1050.203725	10.356564	69.123559
1049.187342	10.537207	69.128564
1047.957092	16.846562	69.133569
1047.562844	19.525381	69.138574
1046.996297	22.248955	69.143578
1046.844829	11.496602	69.148583
1045.907433	13.884946	69.153588
1045.010488	24.268012	69.158593
1044.615443	18.889034	69.163598
1044.210156	12.332172	69.168602
1043.513581	19.734571	69.173607
1042.142390	25.047680	69.178612
1041.292925	27.232812	69.183617
1041.418085	5.563780	69.188622
1040.645104	17.425168	69.193626
1039.889497	27.090343	69.198631
1039.157733	0.016436	69.203636
1038.738524	19.524662	69.208641
1038.534746	20.011261	69.213646
1037.128436	20.474705	69.218650
1036.197287	17.828617	69.223655
1035.855128	28.840918	69.228660
1035.233683	24.521360	69.233665
1034.273203	22.423967	69.238670
1033.659336	31.989330	69.243674
1033.571313	23.467644	69.248679
1033.068506	28.656805	69.253684
1031.935217	32.992246	69.258689
1031.234703	18.008123	69.263694
1030.556628	17.887382	69.268698
1030.272137	10.193291	69.273703
1029.513374	12.356111	69.278708
1028.597589	19.287204	69.283713
1028.562710	16.211542	69.288718
1027.230575	28.131934	69.293722
1026.879467	21.814024	69.298727
1026.389132	23.604573	69.303732
1025.264618	14.728988	69.308737
1024.543254	17.164970	69.313742
1023.575244	20.406561	69.318746
1023.424754	16.871493	69.323751
1023.003794	16.224167	69.328756
1022.200776	20.568566	69.333761
1021.278121	10.773081	69.338766
1020.527696	19.549640	69.343770
1020.302634	12.748077	69.348775
1019.431641	19.310939	69.353780
1018.446052	23.269661	69.358785
1018.128315	17.752239	69.363790
1017.768991	15.880902	69.368794
1016.846298	19.175207	69.373799
1016.021656	18.615758	69.378804
1015.553959	17.703067	69.383809
1015.283275	16.345887	69.388814
1014.159242	20.485902	69.393818
1013.079843	15.138539	69.398823
1012.833417	9.188746	69.403828
1012.076434	32.918450	69.408833
1011.135389	14.607514	69.413838
1010.329111	23.378772	69.418842
1010.383769	11.412540	69.423847
1010.142174	24.121342	69.428852
1009.017333	25.221239	69.433857
1008.467330	17.960458	69.438862
1007.570952	21.670034	69.443866
1007.101600	9.705172	69.448871
1005.890896	25.926935	69.453876
1005.271790	20.744454	69.458881
1005.087098	4.136092	69.463886
1004.292977	18.038193	69.468890
1003.513488	20.907613	69.473895
1002.679198	13.449224	69.478900
1002.291154	18.055600	69.483905
1002.005532	25.769507	69.488910
1000.726048	23.845877	69.493914
1000.312043	9.055882	69.498919
999.664374	2.671632	69.503924
999.305600	14.880272	69.508929
998.582490	15.222427	69.513934
997.491177	9.564744	69.518938
997.180841	3.420128	69.523943
996.338313	6.648070	69.528948
995.112788	23.211222	69.533953
994.910781	11.839315	69.538958
994.065694	21.438310	69.543962
993.924793	16.408402	69.548967
993.022432	19.436140	69.553972
992.384726	20.884302	69.558977
992.072448	12.753108	69.563982
991.092035	15.351734	69.568986
990.451198	17.847450	69.573991
989.821821	23.387900	69.578996
989.179113	22.545634	69.584001
988.521459	15.913822	69.589006
987.537766	13.627761	69.594010
987.263502	10.361539	69.599015
986.858640	23.205122	69.604020
985.523140	15.489027	69.609025
984.914875	12.567670	69.614030
984.168794	24.956207	69.619034
984.049272	31.443675	69.624039
983.095667	23.805584	69.629044
982.154343	14.260657	69.634049
981.979916	12.443484	69.639054
981.220423	25.393952	69.644058
980.140733	13.466281	69.649063
979.608818	23.488520	69.654068
978.704809	13.701125	69.659073
978.718075	16.212617	69.664078
978.086178	30.598259	69.669082
977.025791	30.262404	69.674087
976.733103	38.250245	69.679092
976.212148	24.887002	69.684097
975.059088	20.330360	69.689102
974.080924	17.234479	69.694106
973.612575	18.762928	69.699111
973.169578	27.629354	69.704116
972.819029	33.041872	69.709121
971.828426	2.453289	69.714126
970.917615	30.868754	69.719130
970.908135	23.952472	69.724135
969.982659	20.815094	69.729140
969.280848	23.738394	69.734145
968.841545	7.865957	69.739150
968.069808	21.550049	69.744154
967.139299	24.831423	69.749159
966.151596	24.529738	69.754164
965.888106	25.402722	69.759169
965.564568	14.026503	69.764174
964.407610	16.131278	69.769178
963.761780	14.020119	69.774183
963.260603	27.017796	69.779188
962.982301	31.797523	69.784193
962.403833	16.644208	69.789198
961.001023	29.066285	69.794202
960.628931	20.808997	69.799207
960.197838	22.208523	69.804212
959.251511	25.432496	69.809217
958.702215	22.970098	69.814222
957.591246	14.820919	69.819226
957.214239	12.788409	69.824231
956.917016	12.258596	69.829236
955.834281	20.074103	69.834241
955.457810	13.528445	69.839246
954.763895	25.616962	69.844250
954.329347	16.828742	69.849255
953.313320	16.933676	69.854260
952.582935	16.925354	69.859265
952.559864	14.532188	69.864270
951.232565	23.334323	69.869274
950.636557	13.819619	69.874279
950.046087	21.876910	69.879284
949.406403	11.175452	69.884289
949.016454	17.043648	69.889294
947.710297	24.766982	69.894298
947.532865	13.973047	69.899303
947.353828	30.951580	69.904308
946.471141	14.526822	69.909313
945.841896	15.845920	69.914318
944.649326	11.592039	69.919322
943.879885	15.204167	69.924327
943.228568	25.262756	69.929332
942.837745	18.884956	69.934337
942.582295	10.115552	69.939342
941.147714	31.430051	69.944346
940.678351	16.743490	69.949351
940.187058	13.038741	69.954356
939.718896	8.898244	69.959361
939.015268	12.340636	69.964366
937.881072	19.233971	69.969370
937.208224	20.550548	69.974375
937.183915	12.622693	69.979380
936.378413	24.585470	69.984385
935.673714	21.641625	69.989390
934.912564	15.858898	69.994394
934.552565	17.816373	69.999399
933.116655	16.550003	70.004404
932.347916	24.760240	70.009409
932.305990	13.861170	70.014414
931.730081	23.459923	70.019418
931.290042	17.542526	70.024423
930.068389	13.670156	70.029428
929.616728	25.368481	70.034433
929.152401	22.890994	70.039438
928.347477	21.071654	70.044442
927.716701	10.624242	70.049447
926.999333	11.495338	70.054452
926.401561	26.444809	70.059457
925.938433	15.986486	70.064462
924.768717	15.683819	70.069466
924.419525	10.576683	70.074471
923.581967	17.460666	70.079476
922.219324	22.154330	70.084481
922.231143	8.927106	70.089486
921.509829	20.146386	70.094490
921.375021	17.742617	70.099495
920.834168	13.843917	70.104500
919.870271	18.767431	70.109505
919.359072	21.237804	70.114510
918.336789	19.476709	70.119514
917.781929	12.103195	70.124519
916.931174	20.506249	70.129524
916.402299	24.439637	70.134529
915.861444	18.721205	70.139534
914.707674	25.903084	70.144538
914.254954	20.128051	70.149543
914.041676	21.078201	70.154548
913.082896	30.679543	70.159553
912.196385	18.535092	70.164558
911.492311	20.395941	70.169562
911.327156	18.261919	70.174567
911.037244	21.636907	70.179572
909.843088	23.339211	70.184577
909.105885	14.242790	70.189582
908.671392	25.367550	70.194586
907.763681	15.730580	70.199591
906.660211	22.803536	70.204596
905.867085	17.522628	70.209601
905.793280	24.046969	70.214606
905.448549	9.783700	70.219610
904.984460	22.516865	70.224615
904.309489	13.087280	70.229620
903.516271	36.387538	70.234625
902.365429	12.724967	70.239630
901.441171	20.190434	70.244634
900.972415	16.535721	70.249639
900.627305	20.785206	70.254644
900.016671	28.210230	70.259649
899.523004	15.968580	70.264654
898.588508	17.352035	70.269658
898.158950	7.456065	70.274663
897.253553	26.548096	70.279668
896.214350	6.810003	70.284673
895.994818	24.075653	70.289678
895.559682	7.198100	70.294682
894.717566	29.288770	70.299687
893.723998	20.136958	70.304692
893.336326	16.615994	70.309697
892.814851	15.035399	70.314702
891.641198	16.188844	70.319706
890.967903	32.739847	70.324711
891.011650	29.211724	70.329716
889.961511	15.614202	70.334721
889.305329	21.693501	70.339726
888.233151	26.681566	70.344730
888.011067	17.559943	70.349735
887.690048	23.660019	70.354740
886.643741	24.066254	70.359745
886.048255	16.047957	70.364750
885.274123	16.767256	70.369754
884.885638	11.426693	70.374759
884.154361	27.535928	70.379764
883.303872	22.879143	70.384769
883.102514	8.313957	70.389774
882.200872	11.981831	70.394778
880.974940	21.441195	70.399783
880.149372	7.473647	70.404788
879.755927	18.319068	70.409793
879.721407	25.262917	70.414798
879.092186	20.219274	70.419802
878.055877	1.871556	70.424807
877.512297	16.575862	70.429812
876.792853	23.464715	70.434817
876.199085	9.203244	70.439822
875.144138	21.598373	70.444826
874.564005	8.927392	70.449831
874.504515	10.464902	70.454836
873.412253	28.763543	70.459841
873.164608	11.461932	70.464846
872.409891	19.939595	70.469850
871.555015	19.571079	70.474855
870.638259	16.604235	70.479860
869.971042	9.895143	70.484865
869.846495	8.700797	70.489870
868.541422	28.286934	70.494874
867.941938	-3.202712	70.499879
867.222253	23.895586	70.504884
866.805289	33.368136	70.509889
866.592199	10.674369	70.514894
865.393298	23.865089	70.519898
864.700180	19.377224	70.524903
864.806324	26.919981	70.529908
863.828548	21.353096	70.534913
863.348359	22.866103	70.539918
862.554958	2.328856	70.544922
861.512848	28.787800	70.549927
860.586982	18.726402	70.554932
859.775240	17.354431	70.559937
859.657705	12.962615	70.564942
859.233919	17.984685	70.569946
858.382737	15.851046	70.574951
857.721641	13.546811	70.579956
857.218970	24.450621	70.584961
856.315530	5.160861	70.589966
855.341729	35.666280	70.594970
854.750694	23.583632	70.599975
854.503524	4.380230	70.604980
853.351085	36.276513	70.609985
852.591420	17.829569	70.614990
851.718376	31.589733	70.619994
851.451319	2.999117	70.624999
851.156156	33.051184	70.630004
850.938035	13.078356	70.635009
850.189496	7.441884	70.640014
849.093419	23.167649	70.645018
848.798370	14.762517	70.650023
847.774413	7.700220	70.655028
846.756712	39.343263	70.660033
846.722616	-2.517687	70.665038
845.429238	23.153374	70.670042
845.061202	-6.821427	70.675047
844.097974	38.662747	70.680052
844.078289	7.085544	70.685057
843.490441	27.306556	70.690062
842.203334	-0.946664	70.695066
841.870132	27.480942	70.700071
841.023160	6.783500	70.705076
840.283300	-4.509065	70.710081
839.669756	29.967951	70.715086
838.761864	13.898909	70.720090
838.807350	13.268836	70.725095
837.977496	2.484156	70.730100
836.888263	37.631388	70.735105
836.602075	14.607073	70.740110
835.947345	15.170193	70.745114
835.104873	2.533102	70.750119
834.306016	26.334118	70.755124
833.988739	22.015092	70.760129
833.464640	12.408563	70.765134
832.263143	33.678118	70.770138
831.841662	18.044146	70.775143
831.345295	10.894729	70.780148
830.706537	20.643839	70.785153
830.134255	17.366727	70.790158
829.168673	23.345479	70.795162
828.512267	9.212263	70.800167
828.003664	37.910646	70.805172
826.724507	13.896405	70.810177
826.485022	15.240224	70.815182
826.078768	19.789595	70.820186
825.285214	35.635955	70.825191
824.611981	0.095996	70.830196
823.690862	22.747994	70.835201
823.462904	15.281476	70.840206
823.102632	18.099989	70.845210
821.820507	15.941918	70.850215
821.413286	7.157275	70.855220
820.520753	29.754273	70.860225
820.337015	18.280146	70.865230
819.248465	15.555124	70.870234
818.596823	21.447641	70.875239
818.286326	16.791663	70.880244
817.167861	27.307811	70.885249
816.367860	11.011885	70.890254
815.686006	26.887765	70.895258
815.360590	26.323035	70.900263
814.833216	15.613208	70.905268
813.471200	30.887754	70.910273
813.222556	17.742995	70.915278
812.598914	24.476270	70.920282
812.404599	15.460625	70.925287
811.452041	24.125905	70.930292
810.510776	26.805096	70.935297
810.127788	7.289021	70.940302
809.790157	12.902907	70.945306
808.715251	19.271211	70.950311
808.076615	15.413334	70.955316
807.529987	28.981205	70.960321
806.630341	10.627535	70.965326
805.790172	19.476766	70.970330
805.244058	11.286643	70.975335
804.795628	14.388838	70.980340
804.498516	32.720198	70.985345
803.866542	15.093440	70.990350
802.536956	20.912529	70.995354
802.040884	25.829425	71.000359
801.889972	17.754582	71.005364
800.329001	21.033867	71.010369
800.140729	16.471973	71.015374
799.576722	11.966734	71.020378
798.876395	37.436203	71.025383
798.068694	20.625858	71.030388
797.015577	15.111997	71.035393
796.974912	25.221634	71.040398
796.445937	24.455928	71.045402
795.531669	9.849706	71.050407
794.852122	32.264580	71.055412
794.490196	25.355530	71.060417
793.851491	14.296017	71.065422
792.762291	20.288149	71.070426
791.971581	21.005384	71.075431
791.787791	7.200639	71.080436
790.922471	18.490168	71.085441
790.263626	7.104298	71.090446
789.339896	20.479887	71.095450
788.941706	17.916212	71.100455
788.507901	12.522962	71.105460
787.341875	21.392531	71.110465
786.818584	21.950510	71.115470
786.431400	29.885587	71.120474
785.659833	22.644371	71.125479
784.709155	15.163599	71.130484
783.761018	22.364830	71.135489
783.624463	12.322904	71.140494
783.225371	19.796267	71.145498
782.654096	25.176126	71.150503
782.039334	17.432156	71.155508
780.798750	19.594476	71.160513
780.252590	11.628286	71.165518
779.279771	40.223951	71.170522
779.008716	12.983800	71.175527
778.870060	25.887510	71.180532
778.219423	21.906977	71.185537
777.288245	19.530645	71.190542
776.621597	18.834166	71.195546
775.650989	12.018865	71.200551
775.040239	25.404562	71.205556
774.231314	15.606856	71.210561
773.949889	5.329388	71.215566
772.904323	18.290730	71.220570
772.192078	23.751375	71.225575
771.815456	16.981863	71.230580
771.139431	21.891139	71.235585
770.718027	13.843592	71.240590
769.408895	33.608600	71.245594
769.019950	22.066226	71.250599
768.793710	12.139500	71.255604
767.655927	16.743829	71.260609
766.924224	19.630937	71.265614
766.232772	22.027534	71.270618
765.967583	20.507090	71.275623
765.628563	1.233190	71.280628
764.290079	16.166539	71.285633
763.808068	14.802032	71.290638
763.330700	24.922839	71.295642
762.640460	19.340189	71.300647
762.012522	7.009585	71.305652
760.879366	29.378400	71.310657
760.554859	21.463655	71.315662
759.231650	7.155933	71.320666
758.757402	23.684712	71.325671
758.373228	16.069615	71.330676
757.701286	11.192080	71.335681
757.740425	21.372580	71.340686
756.849289	20.260854	71.345690
755.932871	8.088134	71.350695
755.533379	10.118146	71.355700
754.493725	29.148000	71.360705
753.732528	0.300217	71.365710
753.352071	17.936801	71.370714
752.722472	16.830747	71.375719
752.446220	7.426055	71.380724
751.170759	14.704631	71.385729
750.878708	8.259118	71.390734
749.827121	13.330681	71.395738
749.135147	9.244781	71.400743
748.622774	-4.045607	71.405748
748.277337	17.328927	71.410753
747.326788	12.524132	71.415758
746.246296	24.402994	71.420762
745.597280	16.973559	71.425767
745.616537	10.368104	71.430772
744.653034	11.641118	71.435777
744.171097	13.975981	71.440782
743.418876	24.692456	71.445786
742.680125	8.834655	71.450791
742.115982	18.478861	71.455796
741.277732	7.746019	71.460801
740.889849	0.891585	71.465806
739.989285	17.936061	71.470810
739.381608	24.439736	71.475815
738.991974	26.417722	71.480820
738.111444	14.360713	71.485825
737.626577	14.997736	71.490830
736.510918	17.332569	71.495834
735.873099	16.459631	71.500839
735.470575	20.704080	71.505844
734.793192	19.307607	71.510849
734.572190	11.406355	71.515854
733.369502	19.755099	71.520858
733.008665	16.387583	71.525863
732.257013	10.291197	71.530868
730.813850	18.949451	71.535873
730.594226	18.845687	71.540878
729.896507	29.785294	71.545882
729.108298	19.866040	71.550887
729.440064	14.907563	71.555892
728.319916	14.273835	71.560897
727.791913	16.146122	71.565902
727.193805	20.576244	71.570906
725.805318	21.754506	71.575911
725.468784	13.680845	71.580916
724.910703	11.779701	71.585921
724.136970	18.229391	71.590926
723.214931	22.318441	71.595930
722.354154	13.811024	71.600935
722.114269	12.338595	71.605940
721.552625	24.495968	71.610945
721.364826	10.748641	71.615950
720.581451	12.092330	71.620954
719.649274	14.301768	71.625959
719.149818	8.761299	71.630964
717.947873	14.957479	71.635969
717.610956	14.900775	71.640974
717.136135	15.236594	71.645978
716.293175	19.281517	71.650983
715.508629	10.104407	71.655988
714.554561	22.089300	71.660993
714.229678	8.746985	71.665998
714.193468	9.668958	71.671002
713.106082	12.650553	71.676007
712.448695	14.445675	71.681012
711.562164	16.682540	71.686017
711.005468	11.535946	71.691022
710.173873	13.227923	71.696026
709.300265	8.246900	71.701031
709.090178	14.721965	71.706036
708.475026	19.187919	71.711041
707.576023	15.683749	71.716046
706.946057	10.522015	71.721050
706.450694	23.531392	71.726055
706.034028	16.019249	71.731060
704.777197	16.709802	71.736065
704.422360	17.941114	71.741070
703.947723	13.134680	71.746074
703.170896	17.049234	71.751079
702.294250	17.974135	71.756084
701.634759	24.271609	71.761089
701.340831	20.835100	71.766094
700.534294	19.199014	71.771098
699.464014	18.637780	71.776103
699.255525	21.482602	71.781108
698.709890	19.396563	71.786113
697.888690	7.919888	71.791118
697.110408	19.028430	71.796122
696.201238	22.405841	71.801127
696.214903	11.928445	71.806132
695.016759	25.013450	71.811137
694.556910	12.656105	71.816142
694.163601	24.100732	71.821146
692.951337	9.253440	71.826151
692.067803	5.910812	71.831156
691.401319	26.579565	71.836161
691.270635	7.792884	71.841166
691.139481	-5.346877	71.846170
690.253811	15.538101	71.851175
689.675882	10.620389	71.856180
688.273248	12.844821	71.861185
687.456657	22.860378	71.866190
686.998626	13.957705	71.871194
686.636842	8.512014	71.876199
685.990208	22.586222	71.881204
685.002556	19.148212	71.886209
684.137571	3.818301	71.891214
683.817988	33.144121	71.896218
683.453129	-0.940490	71.901223
683.037119	30.143136	71.906228
681.605566	-0.199983	71.911233
681.232148	24.342240	71.916238
680.657618	-0.473156	71.921242
679.767184	26.500950	71.926247
679.320728	8.735911	71.931252
678.421484	2.191560	71.936257
678.187386	9.342200	71.941262
677.327543	18.364898	71.946266
676.713762	8.635511	71.951271
676.322161	3.998783	71.956276
675.327447	15.069251	71.961281
674.334170	0.534027	71.966286
673.408099	23.584206	71.971290
673.118230	2.990540	71.976295
673.116682	3.224203	71.981300
672.073521	14.950485	71.986305
671.128353	11.445797	71.991310
670.551541	24.698371	71.996314
670.076529	20.641023	72.001319
669.921330	3.256955	72.006324
668.800534	16.693907	72.011329
668.270121	21.337179	72.016334
667.680886	9.020947	72.021338
666.275460	8.423211	72.026343
665.917554	31.728273	72.031348
665.394968	12.195052	72.036353
665.004877	7.788310	72.041358
664.037050	32.522959	72.046362
663.095471	16.265417	72.051367
662.774950	17.477079	72.056372
662.474630	2.885133	72.061377
661.539466	37.367623	72.066382
660.837621	-0.411581	72.071386
660.326726	24.048455	72.076391
659.765592	16.081530	72.081396
658.360479	29.937491	72.086401
658.042567	-9.791933	72.091406
657.677932	37.309394	72.096410
656.791002	8.626749	72.101415
656.139455	13.090622	72.106420
655.214854	11.897534	72.111425
655.131434	27.635563	72.116430
654.625898	4.535878	72.121434
653.536839	26.815691	72.126439
653.278857	6.081338	72.131444
652.003708	11.839788	72.136449
651.249739	16.110246	72.141454
650.710328	27.092461	72.146458
650.102446	16.012324	72.151463
650.168339	15.203965	72.156468
648.781985	22.989081	72.161473
647.905323	31.875706	72.166478
647.840474	18.247577	72.171482
646.973282	12.795643	72.176487
646.402133	13.922642	72.181492
645.565242	3.274782	72.186497
644.898038	34.010494	72.191502
644.358575	9.342475	72.196506
643.241940	19.260744	72.201511
642.904845	9.889415	72.206516
642.348710	14.193024	72.211521
641.660632	-2.354000	72.216526
640.606889	15.908584	72.221530
640.106210	18.836205	72.226535
639.645596	0.527843	72.231540
639.006884	20.203461	72.236545
638.496220	17.302925	72.241550
637.391454	14.244694	72.246554
636.975372	16.042408	72.251559
636.987119	8.465219	72.256564
635.441766	8.239851	72.261569
635.219567	17.206749	72.266574
634.479853	9.887989	72.271578
633.876699	16.422495	72.276583
633.094914	3.796335	72.281588
632.109857	13.050282	72.286593
631.762318	4.748174	72.291598
631.241268	16.391327	72.296602
629.813440	15.782987	72.301607
629.605812	22.418508	72.306612
628.792881	15.092484	72.311617
628.818787	-0.372955	72.316622
628.315617	11.328845	72.321626
627.264583	28.108744	72.326631
626.501221	13.525883	72.331636
625.549355	15.724296	72.336641
624.891317	14.220700	72.341646
624.511876	14.820456	72.346650
623.782889	16.004133	72.351655
623.482758	18.526098	72.356660
621.965368	14.396648	72.361665
621.570522	28.484385	72.366670
621.525324	20.865799	72.371674
620.739173	8.800130	72.376679
619.928342	13.171109	72.381684
618.907089	19.455247	72.386689
618.479567	17.709948	72.391694
618.219858	15.729777	72.396698
616.712742	26.951251	72.401703
616.514282	14.793568	72.406708
616.104164	21.216917	72.411713
615.218952	16.251969	72.416718
614.515430	22.086559	72.421722
613.850355	23.928660	72.426727
613.748080	27.576553	72.431732
612.698165	30.501764	72.436737
611.957670	18.390975	72.441742
611.441130	25.782137	72.446746
610.440992	17.434149	72.451751
609.495963	10.679505	72.456756
608.843878	26.170634	72.461761
608.642884	21.568212	72.466766
608.337717	12.043579	72.471770
607.308959	22.435125	72.476775
606.737837	20.077212	72.481780
605.927777	25.873580	72.486785
605.335837	15.610902	72.491790
604.202447	14.414815	72.496794
603.488467	33.716102	72.501799
603.256289	-0.071067	72.506804
602.574555	23.399081	72.511809
602.492195	35.108000	72.516814
601.717322	-9.905301	72.521818
600.515035	37.852930	72.526823
600.496939	13.841454	72.531828
599.183787	32.318837	72.536833
598.534795	1.277177	72.541838
597.724121	30.272771	72.546842
597.691538	17.117310	72.551847
597.135064	4.956733	72.556852
596.029263	28.642652	72.561857
595.684815	20.732696	72.566862
595.001970	13.885842	72.571866
593.720645	16.277079	72.576871
593.475735	14.138442	72.581876
592.917792	22.725169	72.586881
591.913134	16.505130	72.591886
591.234736	26.374128	72.596890
590.705074	22.946794	72.601895
590.562487	18.658336	72.606900
589.394603	23.067268	72.611905
588.739069	11.874903	72.616910
587.841359	15.025028	72.621914
587.304060	26.886813	72.626919
587.305973	13.249645	72.631924
586.214706	8.871013	72.636929
585.322483	17.294943	72.641934
584.848987	7.702513	72.646938
583.966019	39.101771	72.651943
583.542107	18.496347	72.656948
582.944855	28.760837	72.661953
582.554456	20.255832	72.666958
581.816725	20.239327	72.671962
580.590624	15.580985	72.676967
580.471608	36.001722	72.681972
579.572879	9.962292	72.686977
578.492960	27.934196	72.691982
577.981490	6.880709	72.696986
577.242185	25.312426	72.701991
577.503407	24.357844	72.706996
576.600359	18.452774	72.712001
575.478817	20.630923	72.717006
575.419822	21.616448	72.722010
573.992838	24.328925	72.727015
573.468889	-3.676620	72.732020
572.870908	31.182642	72.737025
572.604675	7.171283	72.742030
571.598666	19.254363	72.747034
570.977209	16.965975	72.752039
570.559814	7.506534	72.757044
569.954357	13.032211	72.762049
568.807006	12.489618	72.767054
568.098231	19.253838	72.772058
567.417706	17.734916	72.777063
567.360606	30.646122	72.782068
566.120390	20.458320	72.787073
565.466245	14.731224	72.792078
564.982723	11.809038	72.797082
564.523927	21.964746	72.802087
563.768039	12.630175	72.807092
562.836752	7.743549	72.812097
562.339847	12.786758	72.817102
561.998330	5.500797	72.822106
560.669202	16.703404	72.827111
560.312266	17.993414	72.832116
559.525521	20.936650	72.837121
559.099947	7.900564	72.842126
558.614452	20.328081	72.847130
557.752771	9.870277	72.852135
557.060535	5.223112	72.857140
556.528589	17.785753	72.862145
555.917606	20.688380	72.867150
555.358574	8.972904	72.872154
554.550787	15.492709	72.877159
553.933738	17.738742	72.882164
553.227371	13.579507	72.887169
552.620240	6.969759	72.892174
552.119747	11.344942	72.897178
550.850145	20.013484	72.902183
550.069379	2.888351	72.907188
549.548207	13.959119	72.912193
549.295406	21.436007	72.917198
548.951899	-0.040008	72.922202
547.666818	11.174507	72.927207
547.372899	10.705717	72.932212
547.049644	18.942845	72.937217
545.915536	13.423084	72.942222
545.353995	5.572955	72.947226
544.495478	20.030991	72.952231
543.469513	13.371265	72.957236
542.618510	13.997259	72.962241
542.268121	17.765090	72.967246
542.174295	8.692492	72.972250
541.604190	6.447972	72.977255
540.452488	17.795785	72.982260
539.529633	10.239738	72.987265
538.838816	13.445230	72.992270
538.679616	9.764949	72.997274
538.086370	19.189898	73.002279
537.411210	14.705590	73.007284
536.530166	22.701996	73.012289
536.296612	1.053936	73.017294
535.508056	13.115000	73.022298
534.175242	9.350431	73.027303
534.074124	2.708976	73.032308
533.482752	6.862104	73.037313
532.919440	12.866754	73.042318
532.348188	17.349403	73.047322
531.514451	15.337678	73.052327
530.849893	-6.394676	73.057332
530.005119	8.330809	73.062337
529.275229	11.660793	73.067342
528.924907	15.379730	73.072346
527.530767	17.139293	73.077351
527.041658	11.800644	73.082356
527.023868	24.323972	73.087361
526.268358	20.902668	73.092366
525.298288	9.864504	73.097370
523.928063	30.899243	73.102375
524.355901	15.164788	73.107380
523.847777	4.152392	73.112385
522.778795	13.621580	73.117390
521.919645	9.540306	73.122394
521.443240	14.558180	73.127399
520.874705	18.695060	73.132404
519.564288	24.345657	73.137409
519.119782	1.991644	73.142414
518.860096	27.379867	73.147418
518.297932	21.879396	73.152423
517.971057	11.063620	73.157428
516.812358	16.068756	73.162433
515.941197	17.923209	73.167438
515.899404	19.990890	73.172442
514.637706	12.274371	73.177447
514.278678	15.688782	73.182452
513.759865	4.911470	73.187457
512.527825	38.540851	73.192462
512.191328	1.663873	73.197466
511.158019	27.456010	73.202471
511.236345	18.797516	73.207476
510.447686	11.522867	73.212481
509.146622	16.709949	73.217486
508.848582	22.612430	73.222490
508.360551	10.817853	73.227495
507.697491	26.422698	73.232500
506.545131	19.494551	73.237505
506.034334	10.171425	73.242510
505.455126	4.705216	73.247514
505.086425	24.044533	73.252519
504.603372	5.958979	73.257524
503.467854	16.675049	73.262529
502.947735	21.494896	73.267534
502.615101	4.678429	73.272538
501.137805	12.107528	73.277543
500.853693	15.415393	73.282548
500.267343	18.340915	73.287553
499.958817	20.449509	73.292558
498.703495	8.229985	73.297562
498.214917	15.799619	73.302567
498.009846	9.007576	73.307572
497.097671	2.965235	73.312577
495.884071	10.115798	73.317582
495.450014	20.101995	73.322586
494.996201	5.815231	73.327591
494.979284	2.235288	73.332596
493.751385	12.600238	73.337601
493.166396	17.206502	73.342606
492.591115	9.571455	73.347610
491.579959	11.880282	73.352615
491.129358	16.156069	73.357620
490.332626	21.294359	73.362625
489.747091	25.519107	73.367630
488.934632	16.310266	73.372634
488.152349	4.504230	73.377639
488.028646	0.107128	73.382644
487.216156	21.759461	73.387649
486.191279	14.121922	73.392654
485.934754	12.636402	73.397658
485.237393	17.552291	73.402663
484.450710	11.214006	73.407668
483.485077	13.627543	73.412673
483.112134	27.164612	73.417678
482.539675	9.161111	73.422682
481.569267	15.134432	73.427687
480.954425	9.620292	73.432692
480.540372	9.079189	73.437697
479.903448	18.550526	73.442702
479.255436	9.104194	73.447706
478.079356	24.938993	73.452711
477.769496	11.900265	73.457716
477.552096	20.141032	73.462721
476.424017	21.164410	73.467726
475.830182	14.651909	73.472730
474.886173	18.888035	73.477735
474.660213	14.237573	73.482740
474.132969	25.094868	73.487745
472.868605	22.019563	73.492750
472.526436	18.535584	73.497754
472.071314	14.974988	73.502759
471.316326	8.773579	73.507764
470.271052	24.835113	73.512769
469.803403	14.401302	73.517774
469.673550	16.886694	73.522778
468.758772	8.924134	73.527783
467.729503	16.778596	73.532788
467.368950	31.316592	73.537793
467.064948	8.208535	73.542798
466.021903	-4.921521	73.547802
464.992942	8.656965	73.552807
464.461955	14.156606	73.557812
464.073709	17.703405	73.562817
462.941111	14.660728	73.567822
462.184211	6.507449	73.572826
461.994708	15.626823	73.577831
461.695175	17.792332	73.582836
460.895167	17.076188	73.587841
459.849668	12.663519	73.592846
459.650166	9.841183	73.597850
458.640058	17.099688	73.602855
457.785097	8.531543	73.607860
457.108745	12.628842	73.612865
456.541129	19.482556	73.617870
456.453120	12.777519	73.622874
455.404601	14.226604	73.627879
454.619432	23.106581	73.632884
454.087209	15.761138	73.637889
453.659462	9.001423	73.642894
452.581058	15.119686	73.647898
451.815432	23.972898	73.652903
451.475003	11.776371	73.657908
451.054541	21.087078	73.662913
450.134621	8.793650	73.667918
449.684839	4.650342	73.672922
448.950500	16.617635	73.677927
448.148069	22.151066	73.682932
447.428251	10.898038	73.687937
446.705838	14.665226	73.692942
446.405237	7.416923	73.697946
444.895349	18.372423	73.702951
444.547702	18.371079	73.707956
444.226878	18.371769	73.712961
443.609871	16.399660	73.717966
443.044010	2.208035	73.722970
441.831421	8.570018	73.727975
441.598647	9.405043	73.732980
440.959477	10.244893	73.737985
440.202393	9.949251	73.742990
439.527634	5.611563	73.747994
438.691729	23.773266	73.752999
438.411308	10.605285	73.758004
437.332522	17.489981	73.763009
436.534417	15.344886	73.768014
435.840887	13.615196	73.773018
435.635809	8.213974	73.778023
435.160370	2.381186	73.783028
434.221864	14.723192	73.788033
433.436369	11.970567	73.793038
433.235348	13.973734	73.798042
432.038610	17.387584	73.803047
431.272743	18.162471	73.808052
430.956613	16.025740	73.813057
430.479926	14.572149	73.818062
430.089160	13.465975	73.823066
428.989363	19.040480	73.828071
428.529522	8.081918	73.833076
427.711083	13.428675	73.838081
426.576168	19.292614	73.843086
425.986765	12.561814	73.848090
425.588544	14.151719	73.853095
425.412854	17.194746	73.858100
424.539152	18.877754	73.863105
423.571358	23.991280	73.868110
423.137234	15.961619	73.873114
422.271837	22.321913	73.878119
421.569016	13.850960	73.883124
420.846384	15.700702	73.888129
420.389817	20.756430	73.893134
419.941811	15.305606	73.898138
419.098327	13.122018	73.903143
418.450754	9.618905	73.908148
418.106625	9.318974	73.913153
416.639286	17.853503	73.918158
416.062790	12.565073	73.923162
415.558368	17.508582	73.928167
415.219650	20.102944	73.933172
414.882363	15.604263	73.938177
413.492683	11.183380	73.943182
413.249226	11.042443	73.948186
412.656818	11.415977	73.953191
411.405752	6.315451	73.958196
411.075576	13.219643	73.963201
410.522154	19.793571	73.968206
410.175711	7.024033	73.973210
409.202101	18.646276	73.978215
408.610251	15.741386	73.983220
407.984255	14.097134	73.988225
406.930288	9.603842	73.993230
406.226983	3.220769	73.998234
405.523242	13.510123	74.003239
405.430666	2.698049	74.008244
405.203817	13.119566	74.013249
403.607069	19.728851	74.018254
403.282968	16.226237	74.023258
402.800866	4.660980	74.028263
401.561649	6.372272	74.033268
401.049177	13.747037	74.038273
400.484722	7.553143	74.043278
400.328912	21.153375	74.048282
398.749362	17.797186	74.053287
398.375564	14.513795	74.058292
397.988816	2.539127	74.063297
397.322980	17.015369	74.068302
397.118934	8.911213	74.073306
395.804783	9.748241	74.078311
395.132549	19.162142	74.083316
394.946002	9.170825	74.088321
393.183013	15.481765	74.093326
392.845099	7.094603	74.098330
392.174675	16.251183	74.103335
392.053661	18.998507	74.108340
391.560682	3.048104	74.113345
390.560145	15.049937	74.118350
390.237954	9.933875	74.123354
389.645608	10.370479	74.128359
389.090153	14.003850	74.133364
388.242395	7.512918	74.138369
387.073488	19.844345	74.143374
386.788632	7.411914	74.148378
385.747907	4.037686	74.153383
385.112833	2.770185	74.158388
384.649419	12.231231	74.163393
384.122649	11.824795	74.168398
383.653450	9.129017	74.173402
382.204477	19.954999	74.178407
382.151913	15.016736	74.183412
381.796913	-0.674960	74.188417
380.505367	21.534664	74.193422
379.780555	13.485105	74.198426
379.626369	4.963020	74.203431
378.924354	5.462832	74.208436
377.846186	25.679978	74.213441
376.860616	9.005433	74.218446
376.597807	2.591602	74.223450
376.067446	24.907012	74.228455
376.192876	3.849898	74.233460
375.243767	4.572002	74.238465
374.266462	12.331484	74.243470
373.424743	9.144736	74.248474
372.639987	15.665648	74.253479
371.908285	5.813243	74.258484
371.444408	23.428418	74.263489
370.920507	10.138411	74.268494
370.062868	11.412042	74.273498
369.411230	13.201601	74.278503
368.612018	19.507210	74.283508
368.588418	7.618176	74.288513
367.550223	11.705348	74.293518
367.082794	5.185358	74.298522
366.621528	20.100495	74.303527
365.734682	12.745360	74.308532
364.778557	16.827341	74.313537
364.031438	16.861280	74.318542
363.940626	15.732550	74.323546
362.446834	11.098064	74.328551
361.721697	11.076464	74.333556
361.527302	15.511705	74.338561
361.066787	19.472137	74.343566
360.600380	12.669720	74.348570
359.361883	21.270311	74.353575
358.732963	10.871698	74.358580
358.544699	9.715922	74.363585
357.796415	23.875745	74.368590
357.241225	1.463750	74.373594
356.608077	20.868846	74.378599
355.209525	25.893351	74.383604
354.886355	-4.682851	74.388609
353.901678	26.778318	74.393614
353.631841	13.853086	74.398618
353.188253	9.437588	74.403623
352.617038	10.105789	74.408628
351.893514	17.566231	74.413633
350.817586	10.105623	74.418638
350.621253	2.733499	74.423642
349.457355	10.434417	74.428647
348.755555	25.616538	74.433652
348.589051	16.126633	74.438657
347.851907	8.567887	74.443662
346.786805	6.905321	74.448666
346.103807	25.618234	74.453671
345.659511	18.621492	74.458676
345.529837	16.093955	74.463681
344.180554	26.634427	74.468686
343.579171	25.077728	74.473690
343.178867	15.429549	74.478695
342.565974	30.088175	74.483700
341.894275	16.946299	74.488705
340.726613	15.699030	74.493710
340.394688	23.056073	74.498714
340.222668	25.630187	74.503719
339.156040	21.449587	74.508724
338.762551	17.494439	74.513729
337.699245	14.451821	74.518734
337.412165	17.859516	74.523738
336.485821	22.657397	74.528743
335.948168	11.958831	74.533748
335.253189	26.758263	74.538753
333.839371	15.879216	74.543758
333.598060	16.398657	74.548762
332.845997	14.347181	74.553767
332.801328	3.631558	74.558772
332.091637	28.441789	74.563777
330.921034	9.633277	74.568782
330.453484	21.952298	74.573786
329.947965	16.744039	74.578791
329.150416	27.040481	74.583796
328.704415	-3.125071	74.588801
328.041382	39.614741	74.593806
327.458299	16.593775	74.598810
326.635602	-3.888039	74.603815
326.123791	12.763404	74.608820
326.075167	30.192567	74.613825
324.671804	-2.531073	74.618830
323.829493	16.574631	74.623834
322.997659	1.357893	74.628839
322.236617	9.309995	74.633844
321.480436	20.978033	74.638849
320.516761	27.137988	74.643854
320.580423	-4.983691	74.648858
319.982968	18.428869	74.653863
319.692005	22.857427	74.658868
319.375910	2.616555	74.663873
317.923985	34.967454	74.668878
317.790500	13.650415	74.673882
316.259307	-2.424640	74.678887
315.655948	23.811480	74.683892
315.192323	5.656677	74.688897
314.554295	24.143236	74.693902
314.626837	9.320080	74.698906
313.420427	22.855940	74.703911
312.609730	23.696352	74.708916
312.443828	24.437156	74.713921
311.078018	24.848820	74.718926
310.380840	1.344623	74.723930
309.715488	21.896514	74.728935
309.634446	24.476628	74.733940
309.360910	9.915199	74.738945
307.882346	13.899121	74.743950
307.319605	20.477704	74.748954
306.848316	27.513202	74.753959
305.966784	12.715948	74.758964
305.113114	1.232019	74.763969
304.766283	34.996292	74.768974
304.643606	18.239447	74.773978
303.569625	4.721762	74.778983
302.511388	20.263450	74.783988
302.053464	9.534845	74.788993
301.453988	25.061768	74.793998
301.068826	0.049236	74.799002
299.882434	15.426850	74.804007
299.611558	25.161563	74.809012
299.357473	15.606781	74.814017
298.074474	8.846223	74.819022
297.766245	8.753466	74.824026
297.023000	12.101407	74.829031
296.137454	18.248913	74.834036
295.110614	18.291186	74.839041
294.452451	12.072834	74.844046
294.224468	19.571000	74.849050
294.078375	16.166186	74.854055
292.965522	13.702315	74.859060
292.323059	-0.295699	74.864065
291.500846	30.489915	74.869070
290.832834	18.310946	74.874074
289.888529	4.070890	74.879079
289.253136	21.205643	74.884084
289.253903	1.948714	74.889089
288.288985	28.797528	74.894094
287.817641	11.418207	74.899098
286.901324	-3.373477	74.904103
286.509306	20.201875	74.909108
285.551702	-0.903363	74.914113
284.899987	33.614359	74.919118
284.683046	10.875674	74.924122
283.784432	18.496494	74.929127
282.805582	1.324226	74.934132
282.612384	37.328408	74.939137
281.566539	18.354961	74.944142
281.026730	-20.712828	74.949146
280.049076	13.222890	74.954151
279.260887	17.169330	74.959156
279.402346	-15.997566	74.964161
278.379980	26.662281	74.969166
277.334652	9.417027	74.974170
277.129760	-2.037833	74.979175
276.382010	24.301721	74.984180
276.350280	-5.985017	74.989185
275.275070	3.622426	74.994190
274.581949	23.462845	74.999194
273.538092	-7.034714	75.004199
272.540546	4.234995	75.009204
272.202707	33.107925	75.014209
271.595155	-5.343580	75.019214
271.650448	24.387569	75.024218
270.344776	1.964352	75.029223
269.642063	31.456803	75.034228
269.413132	7.247233	75.039233
268.470444	39.988475	75.044238
267.724077	12.649263	75.049242
267.127154	12.241419	75.054247
266.511498	24.232408	75.059252
266.158375	16.019574	75.064257
264.528132	16.880246	75.069262
264.585243	14.333983	75.074266
264.000373	21.512160	75.079271
263.307938	12.113985	75.084276
262.212596	4.419989	75.089281
261.475161	22.633825	75.094286
261.378462	18.235591	75.099290
260.820542	11.657513	75.104295
260.007366	5.673608	75.109300
259.305724	9.029119	75.114305
258.332255	33.173385	75.119310
257.842096	5.113720	75.124314
256.573236	18.126564	75.129319
256.329102	24.368958	75.134324
256.049096	0.107624	75.139329
255.382429	26.746480	75.144334
254.813980	10.336664	75.149338
254.192060	4.848954	75.154343
253.295237	30.975750	75.159348
252.648415	7.892458	75.164353
251.399749	23.587513	75.169358
250.926788	-7.125600	75.174362
250.306834	26.248533	75.179367
250.139738	11.700113	75.184372
249.746411	11.592542	75.189377
248.491149	27.485763	75.194382
248.105083	-5.751595	75.199386
247.682378	23.905932	75.204391
246.397166	-4.559964	75.209396
246.212859	8.207464	75.214401
245.426954	28.672932	75.219406
244.808415	-8.920547	75.224410
243.810122	27.172506	75.229415
243.387584	9.868999	75.234420
243.028817	4.154852	75.239425
242.268531	27.640686	75.244430
241.544471	-2.524651	75.249434
241.065718	19.861364	75.254439
239.851391	5.825217	75.259444
239.115995	26.055561	75.264449
238.413942	8.068095	75.269454
238.272482	11.263359	75.274458
237.701979	21.441626	75.279463
236.502539	3.341071	75.284468
236.318349	28.245724	75.289473
235.395769	11.196960	75.294478
234.877942	0.600928	75.299482
233.888159	17.762210	75.304487
233.141078	4.105730	75.309492
233.032652	5.211096	75.314497
232.123223	3.927448	75.319502
231.304501	0.469021	75.324506
230.224024	22.296553	75.329511
230.127607	7.670646	75.334516
230.257708	-7.126965	75.339521
228.763639	26.608843	75.344526
228.134075	-8.912425	75.349530
227.412904	21.828679	75.354535
226.462092	-3.989313	75.359540
225.927519	19.447914	75.364545
225.401572	0.311230	75.369550
225.026027	12.716503	75.374554
224.728567	1.482978	75.379559
223.603331	14.980691	75.384564
223.212387	16.301396	75.389569
222.237514	23.298911	75.394574
221.225553	6.586092	75.399578
220.479446	8.775504	75.404583
219.945443	4.336606	75.409588
219.814727	18.330192	75.414593
219.242014	4.929760	75.419598
218.173232	-4.339011	75.424602
217.457451	19.546551	75.429607
217.098005	16.199408	75.434612
216.312832	13.684915	75.439617
215.320869	-17.274990	75.444622
215.105142	14.885133	75.449626
214.412433	0.147721	75.454631
213.433633	10.734830	75.459636
212.676056	15.616227	75.464641
211.681274	2.492807	75.469646
211.538313	28.904686	75.474650
211.267571	0.595620	75.479655
210.707561	9.802431	75.484660
210.090521	21.825183	75.489665
209.063239	3.883274	75.494670
208.227660	15.119305	75.499674
207.346913	-9.692747	75.504679
206.658007	27.648756	75.509684
206.871310	2.312210	75.514689
205.778599	4.867524	75.519694
205.007225	13.510396	75.524698
204.129784	18.142835	75.529703
203.836888	3.756407	75.534708
203.519853	14.879815	75.539713
202.321077	24.522764	75.544718
202.067645	17.957659	75.549722
201.277420	9.712028	75.554727
200.203632	14.397844	75.559732
199.651320	21.845218	75.564737
199.014941	4.244679	75.569742
198.708883	2.442255	75.574746
197.622097	28.083695	75.579751
197.113668	-6.357786	75.584756
196.770143	38.779948	75.589761
195.640319	15.336878	75.594766
195.228952	-10.046710	75.599770
194.389744	30.174479	75.604775
193.765540	4.000090	75.609780
193.212683	11.084865	75.614785
192.380498	17.329545	75.619790
192.208125	-12.460088	75.624794
191.239606	12.298344	75.629799
190.246617	-9.439816	75.634804
189.630410	7.611448	75.639809
189.090454	-1.137671	75.644814
188.624634	10.537706	75.649818
187.595732	-10.839927	75.654823
186.984622	3.424182	75.659828
186.615544	19.713854	75.664833
186.326507	0.769642	75.669838
185.560599	14.821910	75.674842
184.764121	5.140750	75.679847
183.912324	5.536768	75.684852
183.310305	3.593880	75.689857
182.298193	1.088774	75.694862
181.551021	1.537496	75.699866
181.512892	19.105288	75.704871
180.623268	4.331475	75.709876
179.999370	-2.540391	75.714881
178.972578	22.151659	75.719886
178.834507	-11.647132	75.724890
178.274508	10.040647	75.729895
177.288208	13.960354	75.734900
176.698250	1.161905	75.739905
175.830393	8.765233	75.744910
175.338636	-2.872519	75.749914
174.233858	6.072655	75.754919
173.536488	2.416716	75.759924
173.488533	0.461188	75.764929
172.797196	9.791438	75.769934
172.119118	5.183143	75.774938
171.289929	10.776099	75.779943
170.634865	10.637733	75.784948
170.628541	5.827729	75.789953
169.282268	4.668941	75.794958
168.500778	11.757057	75.799962
168.027785	8.599906	75.804967
167.491561	7.851266	75.809972
166.717906	-4.290291	75.814977
166.003481	17.953526	75.819982
165.347167	2.543312	75.824986
164.958630	1.706475	75.829991
164.049981	15.931308	75.834996
163.536610	5.159552	75.840001
162.913502	13.190620	75.845006
161.956342	5.083581	75.850010
161.100886	13.705177	75.855015
160.272854	4.133133	75.860020
160.542343	1.702815	75.865025
159.850171	13.628740	75.870030
158.873999	1.183595	75.875034
158.201295	-0.399527	75.880039
157.767687	9.329583	75.885044
156.908681	14.769610	75.890049
155.512349	4.882917	75.895054
155.252421	0.925440	75.900058
154.916906	16.875458	75.905063
154.356854	-1.757461	75.910068
153.209700	-3.298051	75.915073
152.396962	16.872081	75.920078
152.265082	10.606138	75.925082
151.916158	6.333281	75.930087
150.851930	5.744518	75.935092
150.338562	20.852461	75.940097
149.542198	8.865901	75.945102
149.436375	-2.469115	75.950106
148.348168	21.016959	75.955111
147.400343	9.986482	75.960116
147.264849	17.805777	75.965121
146.130259	9.610343	75.970126
145.079825	1.708988	75.975130
145.028336	19.870233	75.980135
144.484651	20.737509	75.985140
143.882974	11.178261	75.990145
142.801209	7.769689	75.995150
142.273424	6.677527	76.000154
141.818050	15.060306	76.005159
140.687262	18.377045	76.010164
140.526233	2.231893	76.015169
139.817335	1.570712	76.020174
138.975374	29.279833	76.025178
138.193292	-0.552932	76.030183
137.194761	17.437624	76.035188
137.062526	9.276334	76.040193
136.361788	13.480092	76.045198
136.067922	-1.658327	76.050202
134.956608	28.744466	76.055207
134.200405	7.654505	76.060212
133.912648	27.498111	76.065217
132.704080	3.788552	76.070222
132.121878	10.263034	76.075226
131.817801	13.067934	76.080231
131.245902	2.707625	76.085236
130.591130	7.344002	76.090241
129.612206	12.913539	76.095246
129.155111	6.768836	76.100250
128.751859	1.361414	76.105255
127.737432	16.516131	76.110260
127.201390	2.226839	76.115265
126.463241	14.051296	76.120270
125.477613	8.940145	76.125274
124.776104	13.177143	76.130279
124.138749	17.269879	76.135284
124.017162	0.367851	76.140289
123.454013	19.801216	76.145294
122.397765	11.158085	76.150298
121.926336	10.799650	76.155303
120.965017	15.592137	76.160308
120.830029	9.170583	76.165313
119.887712	15.896444	76.170318
119.260773	10.387499	76.175322
119.136158	9.136444	76.180327
117.850477	22.621934	76.185332
117.120152	12.843523	76.190337
116.482905	4.545154	76.195342
116.012503	2.661718	76.200346
115.027270	13.041735	76.205351
114.252901	3.683494	76.210356
114.002548	6.227528	76.215361
113.289820	21.412991	76.220366
112.325877	0.794549	76.225370
111.346138	29.918021	76.230375
111.051828	-0.429298	76.235380
111.002363	20.822294	76.240385
110.094602	10.920798	76.245390
109.409996	13.010554	76.250394
108.549734	3.634475	76.255399
108.053472	21.322614	76.260404
107.354339	9.815708	76.265409
106.230099	6.117475	76.270414
105.878133	20.152638	76.275418
105.988294	5.916421	76.280423
104.360065	15.328273	76.285428
104.029381	4.495869	76.290433
103.585056	19.674802	76.295438
102.949954	8.227072	76.300442
101.764064	8.326324	76.305447
101.004814	9.344671	76.310452
101.020816	21.075690	76.315457
99.892613	16.094511	76.320462
99.123954	5.592131	76.325466
98.760115	17.992389	76.330471
98.294841	18.262151	76.335476
97.605089	11.046010	76.340481
96.411337	10.848490	76.345486
96.198391	15.725068	76.350490
95.684853	8.070843	76.355495
94.468506	12.656435	76.360500
93.898979	17.376996	76.365505
93.231135	24.904308	76.370510
93.051945	0.749957	76.375514
92.027771	29.860017	76.380519
91.193900	-2.134239	76.385524
90.762991	12.433874	76.390529
90.221333	15.483233	76.395534
89.580384	-2.972761	76.400538
88.599933	9.059061	76.405543
88.076819	-0.008087	76.410548
87.927765	2.653829	76.415553
86.826452	20.968280	76.420558
86.014753	-4.039209	76.425562
85.474483	23.957669	76.430567
84.872037	-4.900803	76.435572
83.930826	18.962364	76.440577
83.512389	-1.298367	76.445582
82.946505	38.503952	76.450586
82.326749	13.782778	76.455591
81.601057	-17.451288	76.460596
80.845993	0.736966	76.465601
80.387445	40.038071	76.470606
79.765846	2.162901	76.475610
78.855584	29.540735	76.480615
78.373958	-1.798512	76.485620
77.718834	36.926835	76.490625
76.349788	9.086253	76.495630
76.091462	-20.391581	76.500634
75.827887	23.173785	76.505639
74.975639	14.272653	76.510644
74.642679	-4.049529	76.515649
73.523385	22.026012	76.520654
72.923175	9.514645	76.525658
72.623371	10.964333	76.530663
71.296854	24.379088	76.535668
71.034913	-24.165735	76.540673
70.270349	26.928673	76.545678
69.579163	18.426036	76.550682
69.102973	15.744055	76.555687
68.043807	22.012353	76.560692
67.984227	4.575346	76.565697
66.550730	-0.363432	76.570702
65.884616	7.207753	76.575706
65.504541	13.645282	76.580711
64.908747	23.971101	76.585716
65.168250	8.132618	76.590721
64.034264	6.243058	76.595726
63.202416	10.756309	76.600730
62.697043	-5.387515	76.605735
61.110680	34.727329	76.610740
60.972788	5.788458	76.615745
60.030898	11.289036	76.620750
59.720209	9.627711	76.625754
59.515226	11.123778	76.630759
58.494515	14.501839	76.635764
58.067241	7.757917	76.640769
57.227316	4.919494	76.645774
56.004562	8.701918	76.650778
55.577845	12.177632	76.655783
54.902541	7.972612	76.660788
54.676649	4.321942	76.665793
53.894084	7.926941	76.670798
53.221370	5.949632	76.675802
52.756558	9.448767	76.680807
51.828794	13.281917	76.685812
50.873656	14.397747	76.690817
50.181288	5.387560	76.695822
49.622933	4.521057	76.700826
49.550917	4.713920	76.705831
48.369014	14.240695	76.710836
47.655800	3.683766	76.715841
47.145535	17.144959	76.720846
46.627281	3.425266	76.725850
45.438345	2.774440	76.730855
44.530918	6.566502	76.735860
44.360196	-2.068000	76.740865
43.908917	-0.608344	76.745870
43.657891	14.208613	76.750874
43.092496	5.635472	76.755879
42.168438	10.095629	76.760884
41.490373	6.494997	76.765889
40.322511	4.678657	76.770894
39.544777	-5.044844	76.775898
39.307895	6.769061	76.780903
38.723304	6.438151	76.785908
38.121565	8.765432	76.790913
37.382204	10.901783	76.795918
36.920182	2.892450	76.800922
36.233792	4.580405	76.805927
34.954777	21.469333	76.810932
34.678871	5.255797	76.815937
33.877932	0.050586	76.820942
33.393480	6.402264	76.825946
32.612241	13.100885	76.830951
31.999919	16.773353	76.835956
31.432086	-6.443816	76.840961
30.551368	24.548222	76.845966
29.899524	4.636950	76.850970
29.717523	-7.748705	76.855975
28.669498	12.812179	76.860980
27.889734	-13.371969	76.865985
27.312972	10.112961	76.870990
26.543481	16.254651	76.875994
26.780092	5.527323	76.880999
25.068747	2.411597	76.886004
24.703878	4.401497	76.891009
24.279021	3.985193	76.896014
23.403513	18.562723	76.901018
22.982073	-1.754272	76.906023
22.047945	4.673857	76.911028
21.455105	15.730873	76.916033
20.783570	9.765471	76.921038
19.916741	3.862756	76.926042
19.632030	18.226217	76.931047
18.990982	11.502206	76.936052
17.850114	-0.219616	76.941057
17.078271	5.884603	76.946062
16.441447	13.648238	76.951066
16.432459	5.527232	76.956071
15.722821	9.459638	76.961076
14.842274	-0.159153	76.966081
14.105045	17.359267	76.971086
13.613423	11.362018	76.976090
12.836154	1.176426	76.981095
11.752759	17.838625	76.986100
11.622826	0.252016	76.991105
11.121635	1.402686	76.996110
10.311226	-1.509809	77.001114
9.420308	7.096978	77.006119
8.691321	13.399360	77.011124
8.514891	-14.743290	77.016129
7.501109	11.878359	77.021134
6.501887	1.723440	77.026139
6.225614	-0.337584	77.031143
5.601687	28.470536	77.036148
4.737619	-9.693869	77.041153
4.188628	22.189801	77.046158