Mon Mar 08 18:38:49 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.180898	112.607581	0.000000
-1.353926	126.010356	0.005005
-2.142725	66.060139	0.010010
-3.266848	4.886387	0.015014
-5.503924	-63.531895	0.020019
-11.209635	-59.941119	0.025024
-17.543545	-6.071022	0.030029
-23.015050	-38.738256	0.035034
-26.488386	-55.625913	0.040038
-30.795372	-8.019160	0.045043
-34.030214	-35.043148	0.050048
-38.074959	-40.864655	0.055053
-41.138116	-50.469523	0.060058
-44.202079	-71.011380	0.065062
-49.015019	-42.303125	0.070067
-52.366148	-23.708655	0.075072
-56.435972	-34.830717	0.080077
-60.162939	-52.482067	0.085082
-63.961078	-36.960561	0.090086
-67.535686	-26.315678	0.095091
-70.991468	-25.065800	0.100096
-74.907954	-32.134511	0.105101
-78.893911	-72.361476	0.110106
-82.448203	-67.347665	0.115110
-86.197354	-53.932766	0.120115
-90.542713	-40.872140	0.125120
-94.088155	-23.030323	0.130125
-97.790256	-20.307737	0.135130
-101.238527	-18.182275	0.140134
-105.318625	-5.283756	0.145139
-109.007647	-13.309601	0.150144
-112.451349	-23.787183	0.155149
-116.474864	-27.423255	0.160154
-120.279789	-42.048682	0.165158
-124.309611	-33.308488	0.170163
-127.885965	-45.705987	0.175168
-131.561450	-49.973110	0.180173
-134.712803	-67.269899	0.185178
-138.723769	-77.838229	0.190182
-142.627245	-77.000917	0.195187
-146.239631	-75.716486	0.200192
-150.707190	-60.792930	0.205197
-154.583367	-19.869738	0.210202
-157.997580	-27.836848	0.215206
-162.269242	-32.100260	0.220211
-165.728617	-58.358072	0.225216
-169.070836	-73.230669	0.230221
-173.199223	-13.354309	0.235226
-176.848089	-32.719383	0.240230
-180.505685	-44.829459	0.245235
-184.414110	-27.235523	0.250240
-187.923488	-60.161762	0.255245
-191.563967	-70.770202	0.260250
-195.462349	-62.985966	0.265254
-199.229642	-42.878955	0.270259
-203.120983	-22.133984	0.275264
-206.833394	-5.200440	0.280269
-210.669165	-20.520939	0.285274
-214.308737	-40.109760	0.290278
-218.742102	-37.913656	0.295283
-222.201194	-40.247247	0.300288
-225.431593	-38.558484	0.305293
-229.205808	-37.273332	0.310298
-232.579281	-59.878526	0.315302
-236.584058	-65.422220	0.320307
-240.421549	-26.569234	0.325312
-244.384667	-12.791940	0.330317
-248.472338	-7.326917	0.335322
-251.941566	-27.393861	0.340326
-256.070994	-55.058371	0.345331
-259.376580	-65.546699	0.350336
-263.099400	-23.050509	0.355341
-267.216712	-41.585329	0.360346
-270.931479	-48.917693	0.365350
-274.156642	-60.662983	0.370355
-277.833444	-72.553778	0.375360
-282.026024	-84.094166	0.380365
-286.203647	-42.167195	0.385370
-289.474636	-26.757888	0.390374
-293.573215	-43.009193	0.395379
-296.982595	-44.156925	0.400384
-300.883145	-42.965030	0.405389
-304.583440	-67.079019	0.410394
-308.469475	-17.743101	0.415398
-312.487351	-30.473513	0.420403
-316.038830	-50.620222	0.425408
-319.235689	-74.153830	0.430413
-323.425768	-32.349367	0.435418
-326.974242	-62.711434	0.440422
-331.045187	-29.655462	0.445427
-335.068689	-51.153849	0.450432
-338.530110	-40.331144	0.455437
-342.493412	-44.971437	0.460442
-345.514636	-69.236329	0.465446
-350.055928	-16.627849	0.470451
-353.618448	-45.393452	0.475456
-356.884707	-66.383494	0.480461
-361.060979	-28.964844	0.485466
-364.742995	-32.860001	0.490470
-368.613494	-53.283673	0.495475
-372.271426	-54.180316	0.500480
-376.315594	-27.718250	0.505485
-380.454531	-42.245745	0.510490
-383.633785	-49.635038	0.515494
-387.745412	-29.321402	0.520499
-391.159625	-63.410411	0.525504
-394.624382	-30.566252	0.530509
-398.513346	-49.782203	0.535514
-402.019097	-47.509957	0.540518
-406.138148	-52.983082	0.545523
-410.042502	-22.659480	0.550528
-413.900104	-49.537652	0.555533
-417.188310	-67.968002	0.560538
-421.075533	-27.618315	0.565542
-425.263770	-47.212188	0.570547
-428.846787	-50.303078	0.575552
-433.161004	-29.078716	0.580557
-436.445084	-35.886687	0.585562
-440.250757	-41.163806	0.590566
-444.207618	-61.806911	0.595571
-447.303639	-36.360280	0.600576
-450.929458	-51.936183	0.605581
-455.160547	-34.468529	0.610586
-458.458299	-60.059397	0.615590
-462.571173	-28.114544	0.620595
-466.332389	-54.328372	0.625600
-470.341035	-47.861697	0.630605
-474.124514	-32.658900	0.635610
-477.309615	-57.006244	0.640614
-481.755365	-43.101089	0.645619
-485.241591	-27.835362	0.650624
-488.869521	-54.472532	0.655629
-492.970984	-42.009974	0.660634
-496.450770	-38.483404	0.665638
-500.288915	-43.198606	0.670643
-504.114394	-43.700880	0.675648
-507.815011	-43.737417	0.680653
-511.533848	-52.678708	0.685658
-514.951647	-35.958979	0.690662
-519.074815	-40.682242	0.695667
-522.980225	-36.564139	0.700672
-526.142410	-72.998501	0.705677
-530.551241	-24.460332	0.710682
-534.056494	-24.794521	0.715686
-538.264796	-30.360391	0.720691
-541.545583	-64.945069	0.725696
-545.220595	-36.138617	0.730701
-548.856079	-32.847285	0.735706
-552.540135	-45.012436	0.740710
-556.746018	-21.545536	0.745715
-560.445790	-68.203488	0.750720
-564.062938	-34.606306	0.755725
-568.244500	-51.080354	0.760730
-571.616880	-36.124428	0.765734
-575.962446	-44.423068	0.770739
-578.990009	-69.014574	0.775744
-583.147588	-23.343767	0.780749
-586.839803	-25.305292	0.785754
-590.230215	-59.247950	0.790758
-594.652753	-23.252958	0.795763
-598.048569	-43.804083	0.800768
-601.927524	-59.001837	0.805773
-605.366482	-28.547348	0.810778
-609.337616	-40.545129	0.815782
-613.238889	-49.496530	0.820787
-616.876904	-28.435092	0.825792
-620.369977	-61.943421	0.830797
-624.373162	-27.108149	0.835802
-627.813214	-62.474588	0.840806
-632.030570	-27.636628	0.845811
-635.805550	-62.020777	0.850816
-639.770771	-25.357664	0.855821
-643.497032	-51.392257	0.860826
-646.979077	-50.425926	0.865830
-650.756033	-24.969622	0.870835
-653.827463	-60.972040	0.875840
-657.851602	-15.997330	0.880845
-662.225705	-52.283607	0.885850
-665.722489	-66.055325	0.890854
-669.735036	-18.543727	0.895859
-673.728200	-23.405756	0.900864
-677.168423	-58.912425	0.905869
-680.981682	-36.913071	0.910874
-684.869008	-41.681605	0.915878
-687.835782	-54.325381	0.920883
-691.695363	-17.806789	0.925888
-695.677421	-60.417314	0.930893
-699.855929	-21.230184	0.935898
-703.323298	-59.684342	0.940902
-707.487819	-24.222394	0.945907
-710.665409	-62.041634	0.950912
-714.853522	-40.507432	0.955917
-718.621859	-42.144365	0.960922
-722.397788	-55.294265	0.965926
-726.232210	-26.019003	0.970931
-729.457575	-72.493794	0.975936
-733.109927	-28.335332	0.980941
-737.438887	-44.862769	0.985946
-740.435804	-68.533310	0.990950
-745.135034	-11.725128	0.995955
-748.263740	-24.557422	1.000960
-752.118102	-45.634213	1.005965
-756.130989	-53.271351	1.010970
-759.893451	-37.543266	1.015974
-763.863103	-59.074647	1.020979
-767.355154	-22.073850	1.025984
-771.096027	-60.509396	1.030989
-774.681180	-29.747524	1.035994
-778.390281	-58.659200	1.040998
-782.584200	-18.840327	1.046003
-786.431348	-43.155496	1.051008
-789.765192	-46.107470	1.056013
-793.536286	-23.102341	1.061018
-797.336839	-74.821143	1.066022
-801.377498	-21.122079	1.071027
-804.853541	-50.717481	1.076032
-809.037422	-40.636485	1.081037
-812.611620	-30.946220	1.086042
-816.476822	-47.241710	1.091046
-819.688790	-67.806047	1.096051
-823.429794	-36.607663	1.101056
-827.697268	-62.329893	1.106061
-831.437363	-27.273071	1.111066
-835.298407	-52.648709	1.116070
-838.771897	-28.599918	1.121075
-842.073569	-57.470952	1.126080
-846.311013	-41.170116	1.131085
-850.354254	-45.814101	1.136090
-853.723113	-58.979957	1.141094
-857.899631	-23.462271	1.146099
-861.406542	-52.672611	1.151104
-865.083439	-39.939883	1.156109
-868.686170	-34.586053	1.161114
-872.236171	-46.806782	1.166118
-876.606718	-17.444025	1.171123
-880.140838	-55.824112	1.176128
-883.678933	-25.869089	1.181133
-888.013432	-37.117616	1.186138
-891.394627	-36.152858	1.191142
-895.567880	-48.787962	1.196147
-899.035692	-29.610898	1.201152
-902.498571	-60.417655	1.206157
-906.456591	-26.932711	1.211162
-910.192265	-49.879400	1.216166
-914.564359	-30.802157	1.221171
-917.765120	-56.004092	1.226176
-921.553575	-21.617462	1.231181
-925.165195	-34.459004	1.236186
-928.953672	-42.346169	1.241190
-932.787492	-36.182641	1.246195
-936.627580	-32.528451	1.251200
-940.263940	-51.083660	1.256205
-944.290250	-37.809280	1.261210
-947.546647	-44.557851	1.266214
-951.589175	-44.121159	1.271219
-955.212446	-59.920511	1.276224
-959.135404	-34.418396	1.281229
-962.979878	-26.548537	1.286234
-966.659060	-61.882419	1.291238
-970.701278	-32.964684	1.296243
-974.020615	-43.178533	1.301248
-977.802513	-40.523845	1.306253
-981.664828	-36.418204	1.311258
-985.243781	-64.457788	1.316262
-989.350791	-13.185681	1.321267
-993.417548	-59.235326	1.326272
-996.905181	-60.733779	1.331277
-1000.674839	-17.127062	1.336282
-1004.192870	-50.192348	1.341286
-1007.943917	-61.239051	1.346291
-1011.495225	-21.655100	1.351296
-1015.659279	-59.199363	1.356301
-1019.581726	-41.349696	1.361306
-1023.111618	-56.848499	1.366310
-1027.037712	-36.771724	1.371315
-1030.653832	-41.822721	1.376320
-1034.189747	-46.503364	1.381325
-1038.306160	-50.387885	1.386330
-1041.885792	-21.365826	1.391334
-1045.686970	-65.507242	1.396339
-1049.842765	-32.272747	1.401344
-1053.220788	-44.096511	1.406349
-1056.829481	-49.512904	1.411354
-1060.895412	-36.252501	1.416358
-1064.514154	-48.012514	1.421363
-1068.096607	-31.838144	1.426368
-1071.928816	-42.346679	1.431373
-1076.086105	-52.989271	1.436378
-1079.516462	-22.163479	1.441382
-1083.458962	-54.861110	1.446387
-1086.608358	-23.536241	1.451392
-1090.696381	-65.376784	1.456397
-1094.912530	-35.773515	1.461402
-1098.285742	-25.047464	1.466406
-1102.580941	-33.454064	1.471411
-1105.553434	-60.169702	1.476416
-1109.415261	-37.433488	1.481421
-1113.469857	-30.236213	1.486426
-1117.126532	-46.676465	1.491430
-1120.921452	-39.616909	1.496435
-1124.352026	-27.281148	1.501440
-1128.266048	-63.253608	1.506445
-1132.541921	-15.437578	1.511450
-1135.855630	-47.101952	1.516454
-1139.759320	-36.144345	1.521459
-1143.583856	-43.979645	1.526464
-1147.165817	-44.571864	1.531469
-1151.037651	-49.722096	1.536474
-1154.601872	-46.461752	1.541478
-1158.692397	-51.912851	1.546483
-1162.824801	-43.566146	1.551488
-1166.024532	-54.554135	1.556493
-1169.712766	-46.363631	1.561498
-1173.167693	-64.401849	1.566502
-1177.125654	-33.885772	1.571507
-1180.990771	-47.794835	1.576512
-1184.840291	-49.891074	1.581517
-1189.029131	-44.688987	1.586522
-1192.226327	-60.923503	1.591526
-1196.121605	-50.301455	1.596531
-1199.875278	-43.727738	1.601536
-1203.565592	-46.666225	1.606541
-1207.541984	-28.091745	1.611546
-1210.806138	-47.907592	1.616550
-1214.860609	-58.981077	1.621555
-1218.605810	-37.641533	1.626560
-1222.596895	-42.264818	1.631565
-1226.359278	-35.864693	1.636570
-1229.513681	-40.114101	1.641574
-1233.857274	-49.737902	1.646579
-1237.819023	-39.726421	1.651584
-1241.343868	-43.735197	1.656589
-1245.328622	-36.179900	1.661594
-1248.679565	-57.872421	1.666598
-1252.380367	-26.914864	1.671603
-1256.286688	-47.736399	1.676608
-1260.060536	-58.867320	1.681613
-1263.723776	-36.919552	1.686618
-1267.849751	-36.656604	1.691622
-1271.899918	-47.768523	1.696627
-1275.345729	-29.113284	1.701632
-1278.604462	-51.988963	1.706637
-1282.480380	-38.643508	1.711642
-1285.764991	-56.040220	1.716646
-1290.284755	-38.704794	1.721651
-1294.054352	-40.121407	1.726656
-1297.893368	-33.365154	1.731661
-1301.906047	-23.253952	1.736666
-1305.178335	-52.461608	1.741670
-1308.742571	-27.882092	1.746675
-1312.343650	-43.280723	1.751680
-1316.392851	-53.638977	1.756685
-1320.285250	-25.673475	1.761690
-1324.098404	-37.433479	1.766694
-1327.677465	-60.005498	1.771699
-1331.603675	-32.493442	1.776704
-1334.844695	-43.512422	1.781709
-1338.937541	-54.625263	1.786714
-1342.845508	-46.925994	1.791718
-1346.735757	-17.314560	1.796723
-1350.221178	-48.413359	1.801728
-1354.058722	-47.308662	1.806733
-1358.118824	-43.926063	1.811738
-1361.589178	-41.509852	1.816742
-1365.537051	-34.179441	1.821747
-1369.361916	-38.207798	1.826752
-1372.938782	-45.107855	1.831757
-1376.742577	-44.290777	1.836762
-1380.148540	-47.596170	1.841766
-1384.116577	-24.591830	1.846771
-1387.953276	-42.589096	1.851776
-1391.629630	-44.802588	1.856781
-1395.523525	-44.967620	1.861786
-1399.189857	-47.457074	1.866790
-1402.958612	-32.960144	1.871795
-1406.818472	-41.670789	1.876800
-1410.732044	-62.266932	1.881805
-1414.313267	-31.609002	1.886810
-1417.754595	-54.992916	1.891814
-1422.023448	-42.800088	1.896819
-1425.324924	-36.263724	1.901824
-1429.277749	-52.305946	1.906829
-1433.387166	-32.323790	1.911834
-1436.819548	-42.966648	1.916838
-1440.665608	-49.129684	1.921843
-1444.293569	-54.326334	1.926848
-1447.969132	-35.766552	1.931853
-1451.868333	-48.236312	1.936858
-1455.555607	-45.559743	1.941862
-1459.556605	-41.725995	1.946867
-1463.424181	-53.026046	1.951872
-1467.105408	-35.936522	1.956877
-1470.480917	-47.614953	1.961882
-1474.210961	-46.002181	1.966886
-1478.218601	-48.162487	1.971891
-1481.968771	-52.089074	1.976896
-1485.378775	-49.691805	1.981901
-1489.675433	-33.044557	1.986906
-1493.238706	-54.005706	1.991910
-1497.245158	-36.403626	1.996915
-1501.117886	-39.440066	2.006912
-1502.323445	-38.406987	2.016909
-1499.377746	-43.116265	2.026906
-1496.548941	-33.330252	2.036902
-1494.280130	-28.675853	2.046899
-1492.515219	-41.330338	2.056896
-1490.481473	-54.443097	2.066893
-1488.957140	-32.827790	2.076890
-1487.222640	-38.151487	2.086886
-1484.847067	-41.972131	2.096883
-1482.958660	-39.931402	2.106880
-1481.387977	-50.750133	2.116877
-1479.281707	-37.442807	2.126874
-1477.363299	-30.932384	2.136870
-1475.466014	-37.308398	2.146867
-1473.469065	-44.039821	2.156864
-1471.609052	-37.578463	2.166861
-1469.679033	-37.546380	2.176858
-1468.056676	-37.733441	2.186854
-1466.176199	-29.357035	2.196851
-1464.125109	-42.581504	2.206848
-1462.375611	-38.514942	2.216845
-1460.320660	-39.271760	2.226842
-1458.315901	-41.672028	2.236838
-1456.550759	-38.102149	2.246835
-1454.484248	-44.078947	2.256832
-1452.877690	-50.392602	2.266829
-1451.044445	-22.337589	2.276826
-1449.205517	-29.575776	2.286822
-1447.152221	-48.141870	2.296819
-1445.353235	-36.079973	2.306816
-1443.377891	-37.275584	2.316813
-1441.429104	-40.707347	2.326810
-1439.746055	-38.737907	2.336806
-1437.506553	-36.677565	2.346803
-1435.987367	-41.488358	2.356800
-1434.093743	-44.994961	2.366797
-1432.155282	-41.062833	2.376794
-1430.245174	-39.080794	2.386790
-1428.158499	-46.993323	2.396787
-1426.536963	-42.674155	2.406784
-1424.763672	-27.671436	2.416781
-1422.710018	-29.154290	2.426778
-1420.807906	-41.565446	2.436774
-1418.820432	-39.884714	2.446771
-1417.249274	-46.538452	2.456768
-1415.110335	-40.952181	2.466765
-1413.435502	-47.859342	2.476762
-1411.524831	-25.630051	2.486758
-1409.206661	-42.336001	2.496755
-1407.551985	-45.314882	2.506752
-1406.001354	-37.662421	2.516749
-1404.039841	-37.602169	2.526746
-1402.306604	-41.626201	2.536742
-1400.211720	-34.521889	2.546739
-1398.149610	-43.333573	2.556736
-1396.312375	-39.516253	2.566733
-1394.614898	-34.160851	2.576730
-1392.687387	-40.645845	2.586726
-1390.698441	-36.860701	2.596723
-1388.811616	-29.007844	2.606720
-1386.867960	-42.802394	2.616717
-1385.037355	-49.346073	2.626714
-1383.336720	-38.815661	2.636710
-1381.501148	-33.359202	2.646707
-1379.415140	-39.009079	2.656704
-1377.359682	-45.722950	2.666701
-1376.058984	-40.487168	2.676698
-1374.019415	-42.491906	2.686694
-1371.873585	-54.713096	2.696691
-1369.998554	-24.905836	2.706688
-1368.509759	-56.560275	2.716685
-1366.320104	-17.121782	2.726682
-1364.301999	-52.006056	2.736678
-1362.317532	-34.659324	2.746675
-1360.708273	-45.673630	2.756672
-1358.976424	-33.297764	2.766669
-1356.851765	-25.203487	2.776666
-1355.419383	-45.305836	2.786662
-1353.358247	-29.622851	2.796659
-1351.447994	-44.240932	2.806656
-1349.315588	-45.254774	2.816653
-1347.400752	-61.858198	2.826650
-1345.602816	-80.024908	2.836646
-1344.003575	-37.841033	2.846643
-1341.915956	-46.186252	2.856640
-1339.799329	-37.634388	2.866637
-1338.213582	-44.195682	2.876634
-1336.568959	-23.202601	2.886630
-1334.325236	-39.277662	2.896627
-1332.554649	-37.607927	2.906624
-1330.406411	-39.011107	2.916621
-1328.825336	-38.310456	2.926618
-1327.145720	-26.368277	2.936614
-1325.000505	-30.344518	2.946611
-1323.037696	-31.506445	2.956608
-1321.248008	-46.370457	2.966605
-1319.308121	-39.467037	2.976602
-1317.688839	-39.282467	2.986598
-1315.638972	-31.103554	2.996595
-1313.639220	-47.881607	3.006592
-1311.653943	-31.733305	3.016589
-1310.047906	-42.949163	3.026586
-1308.597486	-33.621202	3.036582
-1306.362727	-37.779115	3.046579
-1304.185835	-33.256644	3.056576
-1302.541783	-44.759618	3.066573
-1300.613876	-39.935206	3.076570
-1298.498401	-48.021177	3.086566
-1296.774322	-37.137619	3.096563
-1295.127008	-37.620642	3.106560
-1293.077626	-50.031590	3.116557
-1291.108464	-35.723224	3.126554
-1289.353059	-39.302327	3.136550
-1287.581196	-44.668177	3.146547
-1285.762048	-30.406841	3.156544
-1283.605948	-32.755398	3.166541
-1281.994620	-52.654254	3.176538
-1279.900329	-20.862606	3.186534
-1278.010422	-49.164562	3.196531
-1276.522600	-29.022608	3.206528
-1274.444333	-32.421277	3.216525
-1272.294414	-37.271334	3.226522
-1270.935627	-40.502757	3.236518
-1268.372618	-55.552058	3.246515
-1266.853387	-17.125551	3.256512
-1264.834061	-36.821305	3.266509
-1263.096164	-36.423585	3.276506
-1261.350230	-29.916942	3.286502
-1258.995484	-39.375316	3.296499
-1257.745112	-39.943205	3.306496
-1255.818969	-31.384453	3.316493
-1253.600077	-45.342949	3.326490
-1251.636675	-38.383233	3.336486
-1249.945209	-44.014072	3.346483
-1248.098444	-26.946738	3.356480
-1246.194328	-55.361460	3.366477
-1244.622031	-9.304859	3.376474
-1242.622224	-13.481962	3.386470
-1240.425149	-15.930192	3.396467
-1238.654411	-29.482258	3.406464
-1236.526667	-46.036019	3.416461
-1235.390959	-46.547655	3.426458
-1232.873269	-52.667511	3.436454
-1231.274282	-34.619519	3.446451
-1229.426513	-30.819531	3.456448
-1227.333115	-49.859235	3.466445
-1225.603139	-59.785986	3.476442
-1223.758105	-16.419198	3.486438
-1221.790320	-50.676440	3.496435
-1219.940159	-25.944235	3.506432
-1217.863703	-39.764658	3.516429
-1216.286915	-51.075245	3.526426
-1214.314074	-28.307828	3.536422
-1212.144246	-31.313747	3.546419
-1210.654349	-43.534070	3.556416
-1208.676324	-38.221831	3.566413
-1207.153921	-39.987370	3.576410
-1204.916212	-31.233698	3.586406
-1202.986263	-25.973754	3.596403
-1201.086684	-51.342101	3.606400
-1199.040769	-41.539375	3.616397
-1197.623277	-35.117493	3.626394
-1195.412007	-62.733468	3.636390
-1193.740697	-36.662181	3.646387
-1191.881236	-21.728285	3.656384
-1189.919052	-62.566886	3.666381
-1187.864877	-23.608564	3.676378
-1185.929914	-57.195819	3.686374
-1184.426635	-45.391101	3.696371
-1182.641111	-38.745476	3.706368
-1180.700922	-39.952609	3.716365
-1178.213496	-53.324033	3.726362
-1177.038040	-34.112499	3.736358
-1174.849933	-39.475397	3.746355
-1172.901891	-14.652997	3.756352
-1171.275550	-49.043477	3.766349
-1169.078482	-44.696201	3.776346
-1167.424465	-47.889539	3.786342
-1165.696040	-29.852718	3.796339
-1163.343490	-56.368713	3.806336
-1161.856678	-27.719573	3.816333
-1159.862234	-47.321268	3.826330
-1158.323891	-32.148093	3.836326
-1156.092694	-45.066427	3.846323
-1154.260156	-40.842385	3.856320
-1152.409816	-46.501733	3.866317
-1150.321383	-36.576290	3.876314
-1148.637370	-54.396290	3.886310
-1146.835821	-39.585729	3.896307
-1144.818282	-42.668270	3.906304
-1142.976540	-38.740939	3.916301
-1140.679918	-37.110998	3.926298
-1139.318137	-39.040262	3.936294
-1137.280459	-40.785561	3.946291
-1135.331029	-39.087443	3.956288
-1133.476180	-47.497883	3.966285
-1131.991681	-33.066034	3.976282
-1130.064657	-41.140670	3.986278
-1127.827138	-37.294006	3.996275
-1126.201594	-56.198793	4.006272
-1124.210048	-29.133441	4.016269
-1122.343595	-40.259807	4.026266
-1120.483234	-42.112509	4.036262
-1118.718259	-40.695907	4.046259
-1116.657589	-57.276731	4.056256
-1114.822013	-37.283430	4.066253
-1112.609903	-48.120883	4.076250
-1111.052887	-28.676661	4.086246
-1109.314200	-54.226049	4.096243
-1107.557009	-11.539746	4.106240
-1105.523953	-42.038632	4.116237
-1103.441154	-35.779947	4.126234
-1101.952570	-48.918903	4.136230
-1099.764596	-28.931420	4.146227
-1097.910276	-50.359513	4.156224
-1095.860181	-39.433199	4.166221
-1094.263206	-37.571305	4.176218
-1092.341010	-20.391145	4.186214
-1090.460596	-30.016646	4.196211
-1088.554617	-50.313054	4.206208
-1086.504568	-30.554536	4.216205
-1084.834706	-52.437827	4.226202
-1083.255620	-37.877396	4.236198
-1080.731422	-66.245941	4.246195
-1079.281583	-25.144608	4.256192
-1077.244804	-38.660176	4.266189
-1075.628191	-60.097588	4.276186
-1073.617443	-12.149969	4.286182
-1071.277435	-53.598428	4.296179
-1069.869445	-40.311608	4.306176
-1067.980333	-43.108294	4.316173
-1066.099629	-47.744592	4.326170
-1064.222443	-45.790135	4.336166
-1062.438074	-20.148852	4.346163
-1060.383483	-52.924708	4.356160
-1058.311486	-37.683658	4.366157
-1056.711540	-33.499697	4.376154
-1055.376256	-43.858990	4.386150
-1053.036743	-29.202262	4.396147
-1050.716275	-46.561936	4.406144
-1049.279472	-33.920723	4.416141
-1047.245538	-53.354979	4.426138
-1045.230886	-36.211681	4.436134
-1043.622308	-53.383278	4.446131
-1041.481459	-70.128430	4.456128
-1039.745250	-35.618856	4.466125
-1038.158361	-39.323979	4.476122
-1036.041136	-51.826107	4.486118
-1033.871311	-37.925346	4.496115
-1031.972303	-46.356988	4.506112
-1030.464634	-39.587855	4.516109
-1028.914840	-41.761852	4.526106
-1026.702436	-40.989864	4.536102
-1024.760538	-39.882522	4.546099
-1022.861726	-39.276684	4.556096
-1020.878528	-42.140482	4.566093
-1019.159362	-48.416617	4.576090
-1017.505950	-42.802832	4.586086
-1015.733819	-45.141844	4.596083
-1013.202945	-48.653719	4.606080
-1011.538874	-40.783852	4.616077
-1009.615332	-41.986604	4.626074
-1007.855704	-38.622316	4.636070
-1005.975499	-35.035741	4.646067
-1004.481492	-47.322928	4.656064
-1002.323295	-47.887444	4.666061
-1000.281595	-38.922225	4.676058
-998.627249	-45.317449	4.686054
-996.596468	-34.345313	4.696051
-994.520778	-43.817239	4.706048
-993.000843	-45.190688	4.716045
-991.168335	-45.815212	4.726042
-988.921865	-38.335285	4.736038
-987.207442	-37.979392	4.746035
-985.140694	-47.078844	4.756032
-983.433196	-44.688258	4.766029
-981.745426	-45.295945	4.776026
-979.885536	-37.160536	4.786022
-977.941487	-50.405418	4.796019
-975.878663	-46.011222	4.806016
-974.062150	-48.849907	4.816013
-972.199789	-46.725643	4.826010
-970.639174	-42.251136	4.836006
-968.355784	-32.831921	4.846003
-966.428352	-37.702976	4.856000
-964.741588	-30.340354	4.865997
-962.832766	-33.762187	4.875994
-961.338045	-30.499179	4.885990
-959.115619	-32.120717	4.895987
-957.104221	-38.372492	4.905984
-954.973926	-34.454829	4.915981
-953.433758	-29.165496	4.925978
-951.963606	-40.954661	4.935974
-949.635456	-28.091170	4.945971
-948.072472	-30.439323	4.955968
-946.118684	-33.298360	4.965965
-943.734571	-40.413363	4.975962
-941.996257	-33.845245	4.985958
-940.301846	-24.151830	4.995955
-938.631941	-34.624576	5.005952
-936.651316	-36.448999	5.015949
-934.889055	-44.056642	5.025946
-932.788696	-33.243981	5.035942
-930.881196	-30.266413	5.045939
-929.074948	-47.060638	5.055936
-927.446009	-35.496845	5.065933
-925.183448	-38.462071	5.075930
-923.134361	-37.554930	5.085926
-921.566790	-31.712616	5.095923
-919.881922	-31.539834	5.105920
-917.669353	-40.294674	5.115917
-915.924649	-40.418810	5.125914
-914.223044	-36.209948	5.135910
-912.290224	-39.444534	5.145907
-910.167839	-29.705843	5.155904
-908.512977	-31.421322	5.165901
-906.615773	-40.346776	5.175898
-904.544211	-37.649615	5.185894
-902.950165	-32.522012	5.195891
-900.815645	-40.929639	5.205888
-899.167039	-36.641244	5.215885
-897.172206	-32.204523	5.225882
-895.490020	-39.674610	5.235878
-893.643183	-36.663630	5.245875
-891.210958	-43.168936	5.255872
-889.526192	-33.682355	5.265869
-887.908026	-36.743467	5.275866
-885.864841	-34.515413	5.285862
-883.934804	-30.431462	5.295859
-882.172678	-26.953792	5.305856
-880.280204	-46.415859	5.315853
-878.451312	-30.521566	5.325850
-876.586918	-37.866041	5.335846
-874.938855	-42.037133	5.345843
-872.670371	-12.266915	5.355840
-870.774924	-59.208135	5.365837
-869.346730	-20.610345	5.375834
-867.055744	-66.279046	5.385830
-865.247015	-54.936579	5.395827
-863.611525	-25.185181	5.405824
-860.987795	-65.868887	5.415821
-859.809725	-17.966292	5.425818
-857.795697	-45.326357	5.435814
-855.800417	-34.466823	5.445811
-854.056668	-40.386798	5.455808
-851.911235	-42.101713	5.465805
-850.378457	-55.433911	5.475802
-848.616663	-44.636524	5.485798
-846.329560	-17.935427	5.495795
-844.483045	-49.964270	5.505792
-842.902954	-35.964295	5.515789
-841.179035	-24.996629	5.525786
-838.903006	-47.234064	5.535782
-837.184393	-24.482427	5.545779
-835.049136	-45.748456	5.555776
-833.343180	-40.363970	5.565773
-831.547675	-32.666536	5.575770
-829.458989	-47.933291	5.585766
-827.765851	-21.792468	5.595763
-825.824539	-41.985439	5.605760
-824.182894	-28.099486	5.615757
-822.278729	-44.429326	5.625754
-820.256022	-37.639738	5.635750
-818.143091	-50.286272	5.645747
-816.687016	-43.243490	5.655744
-814.359450	-78.186380	5.665741
-812.803695	-71.917399	5.675738
-810.871581	-22.880092	5.685734
-809.003840	-32.561789	5.695731
-807.057745	-44.913245	5.705728
-805.346712	-25.886504	5.715725
-803.365223	-47.819479	5.725722
-801.412937	-18.131267	5.735718
-799.562648	-35.352451	5.745715
-797.761391	-44.186705	5.755712
-796.014209	-49.207229	5.765709
-793.831530	-44.797286	5.775706
-792.209485	-31.110271	5.785702
-790.222647	-49.846871	5.795699
-788.747674	-39.193050	5.805696
-786.219776	-49.581782	5.815693
-784.347767	-46.858935	5.825690
-782.671317	-38.474572	5.835686
-780.974666	-38.679345	5.845683
-778.793893	-28.542503	5.855680
-777.054130	-29.254666	5.865677
-775.508663	-34.790813	5.875674
-773.225589	-59.809703	5.885670
-771.440736	-37.114395	5.895667
-769.687876	-45.303030	5.905664
-768.101985	-33.774854	5.915661
-765.597775	-50.402645	5.925658
-764.085790	-33.091875	5.935654
-762.024409	-43.170780	5.945651
-760.224555	-24.638167	5.955648
-758.240135	-41.394462	5.965645
-756.527552	-44.473733	5.975642
-754.624597	-42.771022	5.985638
-752.532981	-33.679332	5.995635
-750.636552	-47.652207	6.005632
-749.166714	-30.958341	6.015629
-746.984835	-32.656884	6.025626
-745.230696	-41.049384	6.035622
-743.202510	-43.127553	6.045619
-741.424976	-38.016525	6.055616
-739.568990	-44.219609	6.065613
-737.841528	-46.244978	6.075610
-735.798396	-35.358241	6.085606
-734.029260	-40.579593	6.095603
-732.121928	-40.107505	6.105600
-730.098343	-41.007088	6.115597
-728.172825	-39.896880	6.125594
-726.515986	-43.431412	6.135590
-724.663059	-34.892052	6.145587
-722.529585	-34.703976	6.155584
-720.811818	-35.129965	6.165581
-719.067423	-41.649924	6.175578
-717.160276	-32.002956	6.185574
-715.182658	-41.100591	6.195571
-713.180900	-47.622197	6.205568
-711.293454	-33.652279	6.215565
-709.390023	-49.969294	6.225562
-707.660675	-29.788080	6.235558
-705.883156	-37.339595	6.245555
-704.128411	-45.787423	6.255552
-701.859703	-31.213709	6.265549
-700.141682	-30.376623	6.275546
-698.039847	-48.844186	6.285542
-696.844721	-15.862907	6.295539
-694.324741	-48.142978	6.305536
-692.863743	-13.388468	6.315533
-690.970299	-43.490633	6.325530
-689.007099	-52.124907	6.335526
-686.831115	-34.765442	6.345523
-685.180817	-47.127967	6.355520
-683.086288	-46.818376	6.365517
-681.200677	-42.829781	6.375514
-679.561954	-30.209497	6.385510
-677.809931	-41.317282	6.395507
-675.599351	-36.966939	6.405504
-673.636178	-36.644245	6.415501
-672.182623	-53.812996	6.425498
-670.154670	-29.318606	6.435494
-668.201978	-42.326256	6.445491
-666.346170	-40.522785	6.455488
-664.605447	-34.234288	6.465485
-662.814436	-46.644545	6.475482
-660.741389	-42.567465	6.485478
-658.774242	-41.804888	6.495475
-657.015603	-38.053342	6.505472
-654.986787	-38.947382	6.515469
-653.450313	-49.387578	6.525466
-651.209535	-49.800766	6.535462
-649.503060	-35.320320	6.545459
-647.452558	-44.437442	6.555456
-645.715924	-41.340763	6.565453
-644.029045	-39.851323	6.575450
-641.871853	-39.306980	6.585446
-640.371629	-47.159918	6.595443
-638.487436	-37.614999	6.605440
-636.230889	-45.625082	6.615437
-634.622050	-43.089004	6.625434
-632.644834	-42.294858	6.635430
-630.482684	-42.856510	6.645427
-628.859397	-33.975655	6.655424
-627.065433	-41.539216	6.665421
-625.213538	-45.123788	6.675418
-623.098917	-43.183218	6.685414
-621.451572	-42.484778	6.695411
-619.415740	-42.142069	6.705408
-617.504510	-38.845902	6.715405
-615.417310	-33.076905	6.725402
-614.250953	-40.912810	6.735398
-612.202993	-50.211067	6.745395
-609.976011	-33.510157	6.755392
-608.127062	-48.154273	6.765389
-606.261670	-49.756340	6.775386
-604.499818	-43.654323	6.785382
-602.647203	-39.270408	6.795379
-600.628657	-31.849976	6.805376
-598.838367	-44.253766	6.815373
-596.937505	-44.350509	6.825370
-595.315049	-42.121302	6.835366
-593.277198	-25.855920	6.845363
-591.260982	-39.143657	6.855360
-589.233978	-36.925386	6.865357
-587.687932	-48.437556	6.875354
-585.899397	-45.674371	6.885350
-583.817401	-38.571944	6.895347
-581.811835	-48.952831	6.905344
-580.277214	-41.796121	6.915341
-578.033629	-51.847146	6.925338
-576.446286	-43.761004	6.935334
-574.237667	-39.879175	6.945331
-572.428623	-48.330855	6.955328
-570.897750	-34.098592	6.965325
-568.676678	-44.044970	6.975322
-567.100917	-61.053196	6.985318
-564.945649	-45.828095	6.995315
-562.951848	-33.041812	7.005312
-561.275914	-34.102028	7.015309
-559.895725	-55.632500	7.025306
-557.578197	-38.919160	7.035302
-555.626122	-37.370966	7.045299
-553.795078	-17.578446	7.055296
-552.103704	-46.745146	7.065293
-549.790569	-31.725221	7.075290
-548.248984	-38.203202	7.085286
-546.520013	-37.347228	7.095283
-544.186353	-47.152100	7.105280
-542.487480	-26.307464	7.115277
-540.587748	-42.996407	7.125274
-538.828353	-37.909160	7.135270
-536.755077	-32.335223	7.145267
-535.170473	-40.121063	7.155264
-533.430321	-33.909733	7.165261
-531.193339	-38.829898	7.175258
-529.601533	-40.290321	7.185254
-527.595810	-34.934525	7.195251
-525.584747	-38.846013	7.205248
-523.924610	-50.720565	7.215245
-521.784650	-24.652381	7.225242
-520.126472	-43.274753	7.235238
-518.180058	-38.400508	7.245235
-516.141630	-43.159478	7.255232
-514.115170	-39.529539	7.265229
-512.444542	-36.474318	7.275226
-510.631128	-41.655223	7.285222
-508.811507	-42.736771	7.295219
-507.074527	-56.878218	7.305216
-505.146215	-31.617767	7.315213
-503.286812	-51.240109	7.325210
-501.138357	-41.186245	7.335206
-499.498352	-41.664390	7.345203
-497.343037	-44.356315	7.355200
-495.701818	-36.806057	7.365197
-493.659518	-46.889603	7.375194
-491.828787	-46.075103	7.385190
-490.040805	-33.090097	7.395187
-488.172311	-46.568891	7.405184
-486.235583	-40.969947	7.415181
-484.290594	-40.497357	7.425178
-482.455158	-44.161298	7.435174
-480.681471	-43.596615	7.445171
-478.977418	-43.999714	7.455168
-476.711177	-36.715037	7.465165
-474.927739	-37.336065	7.475162
-473.284898	-35.479483	7.485158
-471.327459	-37.655072	7.495155
-469.297447	-43.225783	7.505152
-467.844432	-41.373620	7.515149
-465.468213	-37.575289	7.525146
-463.497460	-36.479981	7.535142
-461.620637	-33.830265	7.545139
-460.205478	-32.038364	7.555136
-457.953198	-32.481627	7.565133
-456.056225	-34.524395	7.575130
-454.516644	-41.155153	7.585126
-453.046866	-35.058472	7.595123
-450.531326	-32.539160	7.605120
-448.467953	-35.500561	7.615117
-447.050222	-38.608324	7.625114
-444.867523	-39.817273	7.635110
-443.080147	-37.159575	7.645107
-440.981126	-37.617821	7.655104
-439.366881	-40.760118	7.665101
-437.544385	-45.885580	7.675098
-435.533222	-44.130415	7.685094
-433.799319	-38.637979	7.695091
-431.592456	-40.599163	7.705088
-429.929335	-41.680925	7.715085
-428.269410	-40.338597	7.725082
-426.442514	-32.295322	7.735078
-424.407019	-34.072828	7.745075
-422.451647	-31.986651	7.755072
-420.550260	-44.820158	7.765069
-418.464280	-34.759387	7.775066
-416.580988	-33.561658	7.785062
-415.193717	-34.079914	7.795059
-413.447139	-41.250520	7.805056
-410.883223	-34.902212	7.815053
-409.303970	-46.923256	7.825050
-407.607629	-31.754163	7.835046
-405.606994	-43.959324	7.845043
-403.516163	-38.429120	7.855040
-401.676136	-37.496039	7.865037
-399.915761	-42.016320	7.875034
-398.428728	-36.610749	7.885030
-396.201229	-38.289419	7.895027
-394.215754	-44.408726	7.905024
-392.400559	-27.701817	7.915021
-390.492105	-40.770111	7.925018
-388.660215	-38.250524	7.935014
-386.814503	-37.032562	7.945011
-384.908855	-38.374058	7.955008
-383.275997	-41.692966	7.965005
-381.099830	-42.386100	7.975002
-379.235283	-37.684971	7.984998
-377.201168	-36.238144	7.994995
-375.682480	-25.709403	8.004992
-373.730919	-43.677518	8.014989
-372.056776	-37.041856	8.024986
-370.024037	-39.464639	8.034982
-367.642535	-31.116715	8.044979
-366.163266	-30.536519	8.054976
-364.490703	-40.963561	8.064973
-362.308792	-36.398344	8.074970
-360.764461	-38.721042	8.084966
-358.524511	-37.442843	8.094963
-356.708841	-34.165936	8.104960
-354.743080	-40.127337	8.114957
-352.843067	-42.014201	8.124954
-351.261188	-33.653865	8.134950
-349.489840	-45.175041	8.144947
-347.558817	-38.779308	8.154944
-345.637281	-36.349785	8.164941
-343.618073	-36.019975	8.174938
-341.654308	-37.430713	8.184934
-340.229489	-34.786106	8.194931
-337.756257	-39.571717	8.204928
-336.138314	-37.771061	8.214925
-334.132497	-34.085562	8.224922
-332.301088	-30.845883	8.234918
-330.585785	-24.469375	8.244915
-328.906755	-35.416884	8.254912
-326.892714	-32.991060	8.264909
-324.722541	-34.186849	8.274906
-322.782393	-34.924356	8.284902
-321.091081	-28.779266	8.294899
-319.428547	-28.029357	8.304896
-317.378723	-31.787401	8.314893
-315.657794	-39.763816	8.324890
-313.573717	-31.584663	8.334886
-311.780310	-30.389869	8.344883
-309.874744	-42.180333	8.354880
-307.993175	-28.602230	8.364877
-306.242927	-29.323621	8.374874
-304.363369	-32.231878	8.384870
-301.826071	-27.611228	8.394867
-300.465862	-28.159834	8.404864
-298.781394	-30.817483	8.414861
-296.751239	-32.474035	8.424858
-295.049434	-33.126110	8.434854
-292.946700	-39.223008	8.444851
-291.265341	-24.760332	8.454848
-289.423533	-32.672349	8.464845
-287.278630	-26.503320	8.474842
-285.466446	-40.942439	8.484838
-283.619220	-39.772003	8.494835
-281.687326	-29.517561	8.504832
-280.021696	-37.592492	8.514829
-277.835870	-38.012349	8.524826
-276.007548	-33.785332	8.534822
-274.034594	-31.614998	8.544819
-272.466078	-33.417313	8.554816
-270.343751	-26.950993	8.564813
-268.665607	-34.145321	8.574810
-266.835317	-32.702180	8.584807
-265.133798	-36.001974	8.594803
-263.070390	-40.639999	8.604800
-260.992179	-41.903156	8.614797
-259.172381	-42.793501	8.624794
-257.310828	-35.780310	8.634791
-255.443682	-29.843226	8.644787
-253.502688	-42.545586	8.654784
-251.796060	-32.471471	8.664781
-249.604897	-48.837286	8.674778
-247.915762	-30.578610	8.684775
-246.129747	-37.648039	8.694771
-244.115393	-44.772853	8.704768
-242.414367	-33.381050	8.714765
-240.294338	-37.401278	8.724762
-238.095032	-43.733008	8.734759
-236.804684	-39.219584	8.744755
-234.985666	-39.639280	8.754752
-232.935822	-47.529191	8.764749
-231.144626	-41.284719	8.774746
-229.215247	-50.559027	8.784743
-227.313167	-36.826242	8.794739
-225.520316	-47.690799	8.804736
-223.477350	-42.479618	8.814733
-221.513339	-43.943981	8.824730
-219.882140	-47.748814	8.834727
-217.907318	-40.974712	8.844723
-216.411861	-50.047136	8.854720
-214.367123	-47.302445	8.864717
-212.563809	-46.759658	8.874714
-210.415462	-42.643660	8.884711
-208.464572	-43.556467	8.894707
-206.764631	-53.116234	8.904704
-204.709306	-45.323960	8.914701
-202.958655	-45.761142	8.924698
-201.147961	-48.797271	8.934695
-199.295228	-36.965453	8.944691
-196.796336	-43.411269	8.954688
-195.810277	-38.572959	8.964685
-193.665231	-37.622077	8.974682
-191.418330	-52.289968	8.984679
-189.972843	-39.177417	8.994675
-187.947929	-51.163673	9.004672
-185.810742	-43.016563	9.014669
-184.265167	-48.931308	9.024666
-182.404291	-39.254371	9.034663
-180.367083	-46.373310	9.044659
-178.524400	-43.405300	9.054656
-176.655467	-45.809679	9.064653
-174.911482	-52.752352	9.074650
-172.877692	-52.060005	9.084647
-171.117831	-53.526486	9.094643
-169.324640	-35.505392	9.104640
-167.371992	-49.188457	9.114637
-165.151200	-48.154904	9.124634
-163.682631	-43.796188	9.134631
-161.722970	-23.794874	9.144627
-159.473859	-40.975111	9.154624
-157.799399	-44.095257	9.164621
-156.119119	-51.092489	9.174618
-154.241021	-38.664703	9.184615
-152.279405	-44.727917	9.194611
-150.501205	-40.417017	9.204608
-148.753438	-45.192473	9.214605
-146.568071	-46.464736	9.224602
-144.516979	-46.763505	9.234599
-142.883959	-37.130700	9.244595
-140.994263	-40.755686	9.254592
-139.240540	-43.315332	9.264589
-137.374846	-32.589163	9.274586
-135.268768	-32.506713	9.284583
-133.629298	-36.151768	9.294579
-131.581087	-37.915272	9.304576
-130.001530	-53.829742	9.314573
-128.079520	-37.385944	9.324570
-125.755649	-34.376247	9.334567
-124.019715	-37.905638	9.344563
-122.204121	-45.469156	9.354560
-120.506597	-33.699340	9.364557
-118.326060	-40.436907	9.374554
-116.754425	-39.195531	9.384551
-114.916118	-44.185928	9.394547
-112.763848	-39.874682	9.404544
-111.077684	-46.310743	9.414541
-109.039691	-45.559014	9.424538
-107.368595	-46.280265	9.434535
-105.404306	-44.272613	9.444531
-103.700217	-44.571248	9.454528
-101.524045	-47.951393	9.464525
-99.792219	-42.311529	9.474522
-97.928205	-46.597095	9.484519
-96.128661	-42.797959	9.494515
-94.188455	-43.336354	9.504512
-92.083356	-39.481755	9.514509
-90.342231	-40.373634	9.524506
-88.355914	-44.334508	9.534503
-86.954233	-25.726676	9.544499
-84.423396	-44.142279	9.554496
-82.792502	-33.822270	9.564493
-80.899869	-41.803826	9.574490
-79.059895	-36.272772	9.584487
-77.411181	-39.341393	9.594483
-75.763121	-36.474878	9.604480
-73.676427	-33.757279	9.614477
-71.408764	-34.990501	9.624474
-69.690844	-32.234595	9.634471
-67.952093	-52.410584	9.644467
-65.631319	-47.990393	9.654464
-64.099109	-42.546017	9.664461
-62.162580	-35.561989	9.674458
-60.493837	-33.033485	9.684455
-58.665054	-33.446713	9.694451
-56.412721	-44.220261	9.704448
-54.736561	-38.078869	9.714445
-52.742669	-46.553379	9.724442
-50.960937	-36.928435	9.734439
-49.429491	-32.521252	9.744435
-47.184782	-35.187577	9.754432
-45.277282	-42.800441	9.764429
-43.301197	-35.132732	9.774426
-41.455493	-36.248093	9.784423
-39.808860	-42.813590	9.794419
-37.879258	-46.896425	9.804416
-36.053971	-41.530357	9.814413
-34.070327	-47.559103	9.824410
-32.004785	-33.893257	9.834407
-30.260841	-37.837531	9.844403
-28.732601	-38.032277	9.854400
-26.517195	-37.532978	9.864397
-24.759611	-32.546083	9.874394
-22.717879	-41.552396	9.884391
-20.787802	-47.201549	9.894387
-19.239477	-34.657881	9.904384
-17.232840	-39.506119	9.914381
-15.305366	-48.461041	9.924378
-13.338608	-44.401155	9.934375
-11.478095	-40.280110	9.944371
-9.771708	-45.884104	9.954368
-7.765801	-43.262506	9.964365
-6.284704	-35.525287	9.974362
-4.887113	-9.369633	9.984359
-3.526166	31.778772	9.994355
-2.280569	87.978399	10.004352
-0.995764	157.291135	10.014349
0.000000	224.126751	10.019354
0.783642	265.646118	10.024359
1.306557	302.123247	10.029363
1.748741	365.198476	10.034368
2.013064	384.806267	10.039373
2.542261	413.000725	10.044378
3.013426	430.945056	10.049383
3.249770	457.357084	10.054387
3.726838	482.316264	10.059392
3.746746	493.022026	10.064397
3.914475	489.623846	10.069402
4.049343	515.153317	10.074407
4.207800	535.621854	10.079411
4.346305	524.958681	10.084416
4.251322	537.920463	10.089421
4.345181	535.991138	10.094426
4.705940	540.814238	10.099431
4.390952	549.608600	10.104435
4.991906	550.099408	10.109440
4.548773	565.277140	10.114445
4.997689	549.440983	10.119450
5.040242	557.746245	10.124455
5.077381	538.664218	10.129459
5.191093	563.112219	10.134464
4.799779	570.956839	10.139469
5.002142	548.223076	10.144474
4.638776	577.544221	10.149479
4.847666	571.920709	10.154483
5.053031	567.956697	10.159488
4.578547	579.088301	10.164493
5.178625	585.816030	10.169498
5.367858	606.295527	10.174503
5.564149	595.217813	10.179507
5.624935	602.898879	10.184512
5.385339	609.147114	10.189517
5.574903	584.942475	10.194522
5.572244	574.612436	10.199527
5.583586	598.297819	10.204531
5.506493	581.698708	10.209536
5.203238	607.079025	10.214541
5.882976	617.072518	10.219546
5.741738	608.068686	10.224551
6.040873	622.809548	10.229555
5.811014	624.120416	10.234560
6.162387	630.897295	10.239565
6.034615	605.172603	10.244570
5.733067	588.689707	10.249575
5.847769	627.593439	10.254579
5.951702	620.220477	10.259584
5.742987	620.178112	10.264589
6.274106	623.393974	10.269594
5.949664	614.599130	10.274599
5.868546	645.826069	10.279603
6.178806	606.890855	10.284608
5.836823	649.220056	10.289613
6.296931	627.477957	10.294618
6.053245	627.647749	10.299623
6.092249	640.104131	10.304627
6.575906	641.596086	10.309632
6.188918	674.791010	10.314637
6.463642	656.561909	10.319642
6.494902	677.069857	10.324647
6.515699	679.067723	10.329651
6.405928	660.431589	10.334656
6.530374	701.754575	10.339661
6.958947	676.250104	10.344666
6.996869	684.210826	10.349671
6.842420	682.947134	10.354675
7.159892	673.590980	10.359680
6.814313	686.998139	10.364685
7.112456	678.700043	10.369690
6.998759	664.784329	10.374695
7.052811	694.944300	10.379699
7.335902	681.223904	10.384704
7.063072	678.908347	10.389709
6.967890	704.443305	10.394714
7.283911	681.330084	10.399719
7.221825	705.811096	10.404723
7.203166	693.950730	10.409728
7.313097	689.765364	10.414733
7.147974	697.310625	10.419738
7.328735	692.584106	10.424743
7.388458	692.058958	10.429747
7.494069	698.100785	10.434752
7.416982	714.628504	10.439757
7.755340	716.585188	10.444762
7.934760	733.529333	10.449767
7.690388	733.505270	10.454771
7.788447	709.261402	10.459776
7.696565	749.431584	10.464781
7.823213	726.055184	10.469786
7.683269	745.768943	10.474791
7.718506	743.069926	10.479795
7.700598	725.161802	10.484800
7.687437	750.380984	10.489805
7.996052	726.218622	10.494810
8.130568	743.696643	10.499815
8.021459	744.920453	10.504819
8.329561	726.446244	10.509824
7.988966	733.524347	10.514829
8.002073	754.536771	10.519834
7.983414	740.221049	10.524839
8.534610	768.261305	10.529843
9.015255	758.376024	10.534848
8.566394	766.255157	10.539853
8.264173	749.556142	10.544858
8.724622	755.539822	10.549863
8.424261	760.567789	10.554867
8.877452	762.823132	10.559872
8.783050	773.671912	10.564877
8.881058	783.871845	10.569882
8.976799	757.004210	10.574887
8.701666	753.263441	10.579891
9.055155	764.211090	10.584896
8.847690	756.130786	10.589901
9.153575	770.474907	10.594906
9.135301	744.529075	10.599911
9.083621	779.015898	10.604915
8.880821	738.093196	10.609920
8.960876	774.266837	10.614925
9.249676	769.086245	10.619930
9.023776	785.254580	10.624935
9.063748	790.110004	10.629939
9.464218	775.287428	10.634944
9.242957	793.017795	10.639949
9.028553	778.268054	10.644954
9.013489	795.325292	10.649959
9.220929	774.727143	10.654963
9.038620	770.260358	10.659968
8.768925	814.737363	10.664973
9.162378	801.954890	10.669978
9.320772	815.166668	10.674983
9.440497	809.644020	10.679987
9.495546	818.657070	10.684992
9.719039	821.603497	10.689997
9.742826	823.980954	10.695002
9.960943	816.663797	10.700007
9.618680	850.809205	10.705011
10.307434	832.450769	10.710016
10.178710	830.252553	10.715021
10.248163	830.943263	10.720026
10.050212	832.991809	10.725031
10.291183	831.549917	10.730035
10.267700	811.042165	10.735040
10.135297	830.373213	10.740045
10.121425	806.348886	10.745050
10.430707	848.689913	10.750055
10.558386	837.255524	10.755059
10.329949	852.355157	10.760064
10.458430	824.975968	10.765069
10.688777	859.271344	10.770074
10.274360	819.862933	10.775079
10.223060	869.730021	10.780083
10.828800	840.918492	10.785088
10.822783	868.816002	10.790093
10.868882	860.706237	10.795098
10.807810	856.647445	10.800103
10.582931	867.583338	10.805107
10.733805	863.962254	10.810112
10.879513	859.577166	10.815117
10.794191	867.713765	10.820122
11.063262	854.383376	10.825127
10.620580	889.710268	10.830131
10.920468	854.234339	10.835136
10.955456	860.505120	10.840141
10.805283	873.621085	10.845146
11.017926	861.099212	10.850151
10.950317	863.262592	10.855155
11.221374	850.605255	10.860160
11.264431	910.928484	10.865165
11.827205	887.083292	10.870170
11.827056	879.086549	10.875175
11.410285	871.468499	10.880179
11.561296	882.369682	10.885184
11.590049	860.040017	10.890189
11.470371	862.544441	10.895194
11.593243	879.259654	10.900199
11.850233	870.734622	10.905203
11.441633	860.555857	10.910208
11.387624	909.617686	10.915213
11.657384	882.971224	10.920218
11.792267	909.717231	10.925223
11.965018	897.499737	10.930227
11.895455	898.941182	10.935232
12.020474	907.495269	10.940237
11.925605	906.775570	10.945242
12.181836	895.719606	10.950247
12.058419	896.523083	10.955251
12.215239	890.032536	10.960256
11.986368	903.331393	10.965261
12.095174	902.084041	10.970266
12.348608	905.085635	10.975271
11.812149	909.433787	10.980275
12.078476	902.717609	10.985280
12.378437	908.865724	10.990285
12.622201	917.927586	10.995290
12.495777	911.013845	11.000295
12.573479	917.618463	11.005299
13.004995	922.050357	11.010304
12.507848	917.152763	11.015309
12.710323	910.222836	11.020314
12.849780	893.219818	11.025319
12.725374	894.294691	11.030323
12.725503	914.106188	11.035328
12.991278	914.366617	11.040333
13.171578	912.806660	11.045338
12.927767	914.372093	11.050343
12.591461	935.798481	11.055347
13.124156	914.577394	11.060352
13.174958	944.757328	11.065357
13.310581	932.335988	11.070362
13.442695	910.503853	11.075367
13.304409	943.654993	11.080371
13.227156	902.741764	11.085376
13.199565	920.367280	11.090381
13.413667	932.643021	11.095386
13.398508	937.570367	11.100391
13.328461	937.289837	11.105395
13.641206	919.163154	11.110400
13.576952	930.969197	11.115405
13.766506	935.026519	11.120410
13.710171	921.334801	11.125415
13.549549	942.912954	11.130419
13.332520	941.947805	11.135424
13.665403	928.903642	11.140429
13.638445	950.480988	11.145434
13.814605	938.010600	11.150439
13.705455	955.245461	11.155443
13.687259	937.770788	11.160448
13.806294	929.617812	11.165453
13.610534	957.796494	11.170458
13.993158	918.483046	11.175463
13.922194	939.230022	11.180467
13.496254	940.583229	11.185472
13.999146	953.478411	11.190477
14.139672	975.360247	11.195482
14.442158	945.778425	11.200487
14.030140	995.998375	11.205491
14.299987	976.591646	11.210496
14.610537	945.838421	11.215501
14.490921	980.156783	11.220506
14.476105	971.063175	11.225511
14.348056	991.155422	11.230515
14.730424	971.872682	11.235520
14.319127	997.677773	11.240525
14.295718	959.871909	11.245530
14.633938	991.521573	11.250535
14.269721	979.134182	11.255539
14.857635	946.674582	11.260544
14.703359	1002.822299	11.265549
14.291696	986.224045	11.270554
15.093088	998.532332	11.275559
14.831335	1006.411715	11.280563
14.961581	1004.596376	11.285568
15.010339	1013.325117	11.290573
15.244229	998.079444	11.295578
15.189453	1021.299815	11.300583
14.645961	1004.372475	11.305587
15.305030	996.664773	11.310592
15.405826	1023.514200	11.315597
15.315542	1003.570351	11.320602
15.731706	990.773052	11.325607
15.435117	1015.837623	11.330611
15.971778	986.169484	11.335616
15.235115	1021.351192	11.340621
16.083451	979.725562	11.345626
16.085610	990.325711	11.350631
15.514605	1027.352887	11.355635
15.588902	1010.889991	11.360640
15.435623	993.108783	11.365645
15.882145	987.093969	11.370650
15.782651	1025.290175	11.375655
15.626169	985.360771	11.380659
15.949460	1005.269088	11.385664
15.680439	989.789813	11.390669
15.753921	1018.747279	11.395674
15.846883	981.367507	11.400679
15.498387	1023.708299	11.405683
15.943756	996.120549	11.410688
15.774618	1010.960148	11.415693
16.127357	1023.073504	11.420698
16.253169	1025.523033	11.425703
16.004015	1036.402999	11.430707
16.722843	1013.032615	11.435712
16.377102	1047.514937	11.440717
16.670245	1018.593638	11.445722
16.465977	1040.018043	11.450727
16.580274	1051.322611	11.455731
16.332777	1020.413798	11.460736
16.688720	1042.403307	11.465741
16.499223	1025.490447	11.470746
16.848935	1040.966430	11.475751
16.553194	1027.919934	11.480755
16.701976	1039.753590	11.485760
16.789152	1046.736810	11.490765
16.930479	1019.541290	11.495770
17.179421	1052.684538	11.500775
16.597295	1036.592817	11.505779
16.895078	1027.646440	11.510784
17.036324	1022.667492	11.515789
17.145955	1031.222529	11.520794
16.794826	1034.588660	11.525799
16.586285	1050.212037	11.530803
16.832063	1032.914349	11.535808
17.118539	1048.465082	11.540813
17.204146	1065.189607	11.545818
17.535502	1066.748480	11.550823
17.549075	1061.282091	11.555827
17.599619	1052.576986	11.560832
17.384137	1078.716850	11.565837
17.490744	1056.259345	11.570842
17.597052	1072.304050	11.575847
17.667281	1049.730928	11.580851
17.967921	1065.918100	11.585856
17.860025	1045.652142	11.590861
17.718423	1069.091446	11.595866
17.829649	1027.362464	11.600871
17.722892	1054.467406	11.605875
17.694812	1067.923626	11.610880
17.847281	1050.852115	11.615885
17.678724	1069.717729	11.620890
18.080877	1069.568471	11.625895
17.881588	1062.579544	11.630899
18.358062	1071.339454	11.635904
18.567977	1055.603947	11.640909
18.051886	1049.919257	11.645914
18.037350	1062.493354	11.650919
18.351374	1063.312230	11.655923
18.265743	1047.360511	11.660928
18.168003	1068.168713	11.665933
18.049455	1055.450331	11.670938
18.363355	1061.366049	11.675943
18.002828	1059.327772	11.680947
18.258612	1057.558638	11.685952
18.168014	1060.179886	11.690957
18.138490	1086.872015	11.695962
18.591271	1094.708449	11.700967
18.528029	1091.476280	11.705971
18.836944	1091.445974	11.710976
18.581660	1098.105360	11.715981
18.701734	1093.295349	11.720986
18.883425	1099.457678	11.725991
19.177219	1091.653640	11.730995
19.372149	1081.439964	11.736000
19.280222	1088.529042	11.741005
18.866379	1096.077906	11.746010
19.114652	1090.962014	11.751015
19.196780	1085.956202	11.756019
19.204087	1092.439661	11.761024
19.182218	1082.982822	11.766029
19.414716	1093.177294	11.771034
19.160818	1080.549864	11.776039
19.135971	1114.884970	11.781043
19.164737	1086.398372	11.786048
19.184105	1107.747786	11.791053
19.311330	1098.240349	11.796058
19.624696	1087.787001	11.801063
19.515828	1122.998140	11.806067
19.465162	1078.618671	11.811072
19.195941	1111.300634	11.816077
19.712442	1099.927032	11.821082
19.933030	1118.349012	11.826087
19.820736	1128.065475	11.831091
20.108908	1133.692004	11.836096
19.904849	1109.375800	11.841101
19.808086	1129.930040	11.846106
20.192616	1119.668751	11.851111
20.097912	1119.917289	11.856115
20.003773	1109.491069	11.861120
20.022120	1123.794667	11.866125
20.041055	1122.479627	11.871130
20.434661	1116.880065	11.876135
19.907163	1127.238350	11.881139
20.291878	1121.607087	11.886144
20.524522	1121.763992	11.891149
20.552858	1128.299308	11.896154
20.706328	1129.353534	11.901159
20.552240	1126.291970	11.906163
20.357852	1118.007521	11.911168
20.631451	1124.849080	11.916173
20.576274	1126.581574	11.921178
20.864479	1112.520903	11.926183
20.278494	1121.890277	11.931187
20.644648	1132.109192	11.936192
20.364393	1134.863207	11.941197
20.492724	1135.957714	11.946202
20.516598	1123.475184	11.951207
20.383325	1120.788780	11.956211
20.678179	1127.339937	11.961216
20.416293	1142.768489	11.966221
20.485491	1153.673465	11.971226
20.811439	1146.253788	11.976231
20.833241	1162.688973	11.981235
20.966257	1167.731540	11.986240
20.790851	1156.461937	11.991245
20.918542	1158.526402	11.996250
21.468136	1165.759214	12.001255
21.565495	1178.185463	12.006259
21.883156	1163.687159	12.011264
21.417322	1162.846833	12.016269
21.552455	1156.089961	12.021274
21.901159	1152.248014	12.026279
21.495432	1148.714054	12.031283
21.578024	1141.779482	12.036288
21.311276	1140.024289	12.041293
21.543452	1154.394742	12.046298
21.371953	1150.706727	12.051303
21.763742	1145.411804	12.056307
22.116378	1134.384440	12.061312
21.918247	1150.179734	12.066317
21.774215	1149.064152	12.071322
21.904010	1120.936699	12.076327
21.735700	1119.780836	12.081331
21.495859	1117.762727	12.086336
21.425327	1110.844706	12.091341
21.506748	1120.415148	12.096346
21.601655	1112.007291	12.101351
21.602643	1126.837223	12.106355
21.795186	1120.246257	12.111360
21.536622	1123.272784	12.116365
21.417042	1121.932525	12.121370
21.664564	1125.327781	12.126375
21.237662	1123.191268	12.131379
21.495693	1121.708781	12.136384
21.549060	1109.958015	12.141389
21.548656	1114.621287	12.146394
21.820517	1126.555236	12.151399
21.757845	1121.230299	12.156403
21.602633	1116.186634	12.161408
21.499108	1101.567115	12.166413
21.163835	1083.346455	12.171418
21.737491	1086.036813	12.176423
21.750494	1088.799242	12.181427
21.391301	1073.678042	12.186432
21.502397	1089.840278	12.191437
21.123599	1097.058693	12.196442
21.511258	1090.655823	12.201447
21.504688	1096.069143	12.206451
21.825591	1085.250309	12.211456
21.580213	1089.165725	12.216461
21.455809	1086.542569	12.221466
21.733341	1088.655668	12.226471
21.515922	1096.852888	12.231475
21.704306	1092.880403	12.236480
21.656437	1095.813396	12.241485
21.783731	1094.798051	12.246490
22.037166	1091.688845	12.251495
21.554487	1083.229617	12.256499
21.570370	1065.672082	12.261504
21.442594	1069.384229	12.266509
21.158341	1065.919227	12.271514
21.431129	1051.898921	12.276519
21.252105	1062.067539	12.281523
21.284666	1086.750147	12.286528
21.555930	1094.677034	12.291533
21.317034	1089.999971	12.296538
21.601056	1089.644044	12.301543
21.835897	1097.523124	12.306547
21.778834	1071.425193	12.311552
21.732624	1065.706557	12.316557
21.492478	1062.923666	12.321562
21.533719	1057.269935	12.326567
21.282669	1074.689999	12.331571
21.230874	1059.021459	12.336576
21.307479	1059.931818	12.341581
21.064114	1064.480856	12.346586
21.355884	1069.570611	12.351591
21.028450	1086.115026	12.356595
21.901903	1088.729185	12.361600
21.630101	1099.538691	12.366605
21.443127	1075.109430	12.371610
21.824917	1059.187230	12.376615
21.284674	1064.299291	12.381619
21.371629	1064.257076	12.386624
21.374335	1059.300211	12.391629
21.108971	1076.314120	12.396634
21.596254	1069.941104	12.401639
21.703988	1070.330823	12.406643
21.693697	1060.515753	12.411648
21.857383	1062.050904	12.416653
21.501698	1071.072848	12.421658
21.811814	1066.778174	12.426663
21.440564	1065.016002	12.431667
21.426890	1073.828856	12.436672
21.502284	1080.255717	12.441677
21.450046	1071.396678	12.446682
21.690157	1073.745983	12.451687
21.355068	1074.884433	12.456691
21.539849	1060.414520	12.461696
21.545727	1071.517195	12.466701
21.262820	1068.466725	12.471706
21.763380	1066.529239	12.476711
21.463808	1070.316095	12.481715
21.682119	1062.733851	12.486720
21.686748	1074.502215	12.491725
21.836784	1066.033552	12.496730
21.473366	1045.038776	12.501735
21.193752	1041.908938	12.506739
21.366175	1042.480732	12.511744
21.617264	1061.337755	12.516749
21.425101	1048.452919	12.521754
21.519580	1037.009475	12.526759
21.350769	1041.524538	12.531763
21.337202	1058.767932	12.536768
21.336414	1049.284098	12.541773
21.099018	1055.836531	12.546778
21.724918	1055.471812	12.551783
21.168909	1074.653121	12.556787
21.656151	1065.889398	12.561792
22.132650	1069.721217	12.566797
21.428073	1062.374475	12.571802
21.360976	1047.796509	12.576807
21.233190	1051.526000	12.581811
21.213973	1036.823712	12.586816
21.688989	1057.630441	12.591821
21.561337	1056.245743	12.596826
21.349262	1048.981311	12.601831
21.039683	1050.748063	12.606835
21.186952	1056.289800	12.611840
21.585706	1071.127200	12.616845
21.369114	1073.161405	12.621850
21.458657	1083.927462	12.626855
21.377264	1083.645585	12.631859
21.473880	1068.965792	12.636864
21.339745	1074.949819	12.641869
21.428534	1065.991018	12.646874
21.593276	1080.656010	12.651879
21.508244	1079.750226	12.656883
21.664092	1074.750008	12.661888
21.385818	1089.228616	12.666893
21.648734	1084.028387	12.671898
21.727883	1076.175010	12.676903
21.419477	1061.433663	12.681907
21.433386	1054.230960	12.686912
21.389784	1048.243827	12.691917
21.046328	1048.558846	12.696922
21.413889	1054.194761	12.701927
21.406768	1078.855299	12.706931
21.332167	1092.831484	12.711936
21.676655	1074.508729	12.716941
21.409713	1080.411435	12.721946
21.547760	1092.562245	12.726951
21.750395	1076.816836	12.731955
21.433066	1057.183519	12.736960
21.138928	1087.108098	12.741965
21.451466	1064.412727	12.746970
21.681005	1085.234991	12.751975
21.468472	1087.255934	12.756979
21.441708	1069.258908	12.761984
21.663292	1055.489621	12.766989
21.365089	1064.568627	12.771994
21.470869	1071.600933	12.776999
21.206937	1070.487133	12.782003
21.397328	1064.702377	12.787008
21.523121	1064.732817	12.792013
21.499829	1063.568022	12.797018
21.475539	1059.008133	12.802023
21.500971	1062.577570	12.807027
21.639710	1062.632754	12.812032
21.856000	1054.429503	12.817037
21.544016	1058.612583	12.822042
22.054460	1047.836088	12.827047
21.421660	1060.619179	12.832051
21.508283	1053.715546	12.837056
21.597293	1054.242295	12.842061
21.220353	1054.964786	12.847066
21.332447	1042.608607	12.852071
21.405254	1055.411624	12.857075
21.099312	1059.032333	12.862080
21.507462	1057.177396	12.867085
21.338426	1065.715397	12.872090
21.430795	1056.241932	12.877095
21.433282	1055.298537	12.882099
21.476618	1057.516792	12.887104
21.459587	1060.369164	12.892109
21.221436	1065.611245	12.897114
21.332927	1059.078966	12.902119
21.185367	1068.219105	12.907123
21.220820	1056.605284	12.912128
21.404775	1064.252759	12.917133
21.047175	1073.724452	12.922138
21.179060	1079.252881	12.927143
20.994995	1108.108096	12.932147
21.856173	1094.951141	12.937152
21.556336	1081.955712	12.942157
21.304512	1109.140665	12.947162
21.722759	1100.580318	12.952167
21.796706	1103.063364	12.957171
21.720005	1089.535589	12.962176
21.556690	1082.039431	12.967181
21.398469	1071.735425	12.972186
21.518815	1059.152406	12.977191
21.615051	1070.824154	12.982195
21.614413	1061.113203	12.987200
21.477712	1067.302643	12.992205
21.617324	1068.489966	12.997210
21.468960	1067.799291	13.002215
21.604775	1072.284702	13.007219
21.524837	1072.253335	13.012224
21.486953	1067.422792	13.017229
21.329818	1072.658262	13.022234
21.617438	1057.031788	13.027239
21.505516	1058.817480	13.032243
21.791845	1070.924122	13.037248
21.819186	1061.782731	13.042253
21.361163	1079.794065	13.047258
22.028533	1065.696621	13.052263
21.981919	1050.771602	13.057267
21.547885	1034.891233	13.062272
21.746570	1036.177943	13.067277
21.494126	1043.434528	13.072282
21.603861	1034.655336	13.077287
21.334081	1039.946608	13.082291
21.286440	1026.578262	13.087296
21.115142	1029.951981	13.092301
20.946078	1033.621818	13.097306
21.540410	1043.036287	13.102311
21.318507	1049.434855	13.107315
21.441080	1046.978902	13.112320
21.576990	1050.092313	13.117325
21.164125	1056.149172	13.122330
21.581703	1048.601387	13.127335
21.347691	1051.253392	13.132339
21.432028	1056.404611	13.137344
21.857549	1052.780679	13.142349
21.460076	1052.697450	13.147354
21.264802	1028.570795	13.152359
21.173575	1044.416735	13.157363
21.250258	1057.482492	13.162368
21.589752	1059.000642	13.167373
21.564448	1069.479070	13.172378
21.590251	1056.529501	13.177383
21.500833	1065.952109	13.182387
21.516621	1058.358012	13.187392
21.486358	1050.570985	13.192397
21.431582	1033.283384	13.197402
21.521827	1033.166526	13.202407
21.622850	1038.813405	13.207411
21.697056	1037.221470	13.212416
21.596459	1041.487528	13.217421
21.521936	1047.980864	13.222426
21.613944	1034.145529	13.227431
21.523541	1038.924057	13.232435
21.311990	1028.410963	13.237440
21.651615	1038.323378	13.242445
21.231258	1048.364893	13.247450
21.336920	1038.389416	13.252455
21.312473	1031.612320	13.257459
21.146442	1034.370176	13.262464
21.214635	1044.343232	13.267469
21.386933	1047.558074	13.272474
21.525153	1041.034156	13.277479
21.276698	1044.702465	13.282483
21.500862	1050.347056	13.287488
21.480413	1051.012690	13.292493
21.225943	1052.748575	13.297498
21.596096	1047.091277	13.302503
21.620356	1051.209689	13.307507
21.335756	1044.587621	13.312512
21.305637	1037.811426	13.317517
21.623098	1057.984104	13.322522
21.418051	1048.663737	13.327527
21.355533	1057.834463	13.332531
21.378396	1057.931782	13.337536
21.765030	1043.262533	13.342541
21.442849	1044.482502	13.347546
21.437377	1042.095857	13.352551
21.448558	1051.300557	13.357555
21.269745	1048.875324	13.362560
21.333450	1047.237753	13.367565
21.426494	1051.471353	13.372570
21.724383	1039.924501	13.377575
21.334323	1047.023260	13.382579
21.465882	1050.591538	13.387584
21.370847	1048.886242	13.392589
21.342505	1048.009265	13.397594
21.423710	1044.403979	13.402599
21.509148	1056.479569	13.407603
21.341280	1059.565736	13.412608
21.231969	1062.306667	13.417613
21.392115	1081.479424	13.422618
21.567463	1086.210853	13.427623
21.780773	1084.978359	13.432627
21.614341	1068.703604	13.437632
21.724905	1054.985141	13.442637
21.495350	1063.157469	13.447642
21.512673	1056.919336	13.452647
21.571047	1059.676101	13.457651
21.333980	1044.863467	13.462656
21.597585	1072.986457	13.467661
21.567193	1062.941196	13.472666
21.762176	1039.151260	13.477671
21.473174	1072.340926	13.482675
21.855123	1062.315060	13.487680
22.050475	1040.420602	13.492685
21.503539	1064.265174	13.497690
21.859423	1060.590844	13.502695
21.370838	1052.488975	13.507699
21.413577	1054.385620	13.512704
21.473034	1038.316151	13.517709
21.099008	1039.533350	13.522714
21.620553	1047.530683	13.527719
21.297082	1053.161690	13.532723
21.325006	1056.637685	13.537728
21.672988	1055.115627	13.542733
21.394776	1059.681260	13.547738
21.446390	1061.633262	13.552743
21.456996	1069.254769	13.557747
21.473903	1051.372228	13.562752
21.431637	1054.408399	13.567757
21.648981	1054.427392	13.572762
21.450232	1047.838940	13.577767
21.456686	1042.111914	13.582771
21.329356	1039.012984	13.587776
21.299876	1041.088306	13.592781
21.529685	1056.589738	13.597786
21.619878	1052.869473	13.602791
21.451194	1049.826022	13.607795
21.422922	1039.023487	13.612800
21.518315	1031.107619	13.617805
21.333290	1038.093246	13.622810
21.652424	1034.864762	13.627815
21.521147	1029.151823	13.632819
21.325051	1033.273834	13.637824
21.560059	1032.305971	13.642829
21.192739	1038.092202	13.647834
21.274735	1028.379132	13.652839
21.074652	1053.272256	13.657843
21.261818	1063.418742	13.662848
21.615429	1068.096502	13.667853
21.523056	1074.632122	13.672858
21.891432	1076.579339	13.677863
21.536159	1059.200857	13.682867
21.713472	1041.316400	13.687872
21.460349	1037.327612	13.692877
21.350639	1039.444116	13.697882
21.797688	1037.570362	13.702887
21.603093	1039.418123	13.707891
21.497476	1031.651010	13.712896
21.929375	1028.183765	13.717901
21.509212	1030.565828	13.722906
21.554643	1024.700126	13.727911
21.548095	1036.217925	13.732915
21.507152	1039.704899	13.737920
21.743048	1032.482573	13.742925
21.562816	1039.571518	13.747930
21.710594	1029.612984	13.752935
21.780251	1034.913197	13.757939
21.233574	1030.137005	13.762944
21.496953	1027.915646	13.767949
21.107060	1034.762055	13.772954
21.547100	1034.914267	13.777959
21.595237	1033.542537	13.782963
21.321128	1035.574871	13.787968
21.483743	1037.504436	13.792973
21.412173	1040.751863	13.797978
21.850622	1037.179490	13.802983
21.055708	1043.962764	13.807987
21.210010	1036.393896	13.812992
21.405118	1035.735177	13.817997
21.596701	1039.189797	13.823002
21.453177	1047.124463	13.828007
21.373420	1055.411671	13.833011
21.570560	1043.082929	13.838016
21.632844	1041.141227	13.843021
21.528568	1038.707262	13.848026
21.478043	1034.618352	13.853031
21.450125	1046.601624	13.858035
21.547771	1034.042749	13.863040
21.374549	1025.600433	13.868045
21.400136	1033.845595	13.873050
21.568715	1027.966559	13.878055
21.693411	1019.839438	13.883059
21.680937	1014.560151	13.888064
21.735273	1009.932543	13.893069
20.952760	1018.795443	13.898074
21.199343	996.605869	13.903079
21.277659	1001.061004	13.908083
21.270334	1027.259044	13.913088
21.722556	1027.366735	13.918093
21.345773	1040.124746	13.923098
21.560875	1016.536646	13.928103
21.545051	1031.063227	13.933107
21.230956	1023.714152	13.938112
21.615581	1024.362490	13.943117
21.364382	1028.505904	13.948122
21.551368	1021.742400	13.953127
21.346870	1007.907070	13.958131
21.021264	1010.636755	13.963136
21.328738	1045.939005	13.968141
21.310841	1045.194407	13.973146
21.496407	1035.671399	13.978151
21.305360	1049.327062	13.983155
21.238424	1036.961594	13.988160
21.479597	1034.018362	13.993165
20.988605	1055.341861	13.998170
21.795664	1034.578324	14.003175
21.436999	1049.342532	14.008179
21.862504	1034.695477	14.013184
21.752745	1063.890421	14.018189
21.464939	1032.568241	14.023207
21.807070	1037.347426	14.028224
21.189505	1049.054424	14.033242
21.696350	1041.785186	14.038259
21.542487	1034.088094	14.043277
21.532430	1049.696671	14.048295
21.518539	1047.852267	14.053312
21.645816	1041.477236	14.058330
21.376451	1043.499023	14.063347
21.736746	1051.364614	14.068365
21.402869	1065.429869	14.073383
21.522693	1040.962222	14.078400
21.649153	1043.170980	14.083418
21.609243	1045.242684	14.088435
21.955940	1054.123434	14.093453
21.481709	1055.567586	14.098471
21.447956	1045.863105	14.103488
21.550297	1046.661616	14.108506
21.424882	1044.834999	14.113523
21.876666	1038.963471	14.118541
21.846454	1044.706496	14.123559
21.410329	1048.406490	14.128576
21.614247	1043.444341	14.133594
21.505264	1046.104339	14.138611
21.776959	1057.210211	14.143629
21.628126	1081.070706	14.148647
21.524195	1084.646946	14.153664
21.869833	1084.112104	14.158682
21.365931	1088.886244	14.163699
21.735441	1082.790302	14.168717
21.754588	1085.981984	14.173735
21.970026	1085.603183	14.178752
21.842329	1098.252948	14.183770
21.920608	1085.312279	14.188787
22.139980	1081.421988	14.193805
21.941183	1092.832580	14.198823
22.109194	1099.424874	14.203840
22.134892	1095.140767	14.208858
21.856258	1089.167069	14.213875
22.082777	1090.364188	14.218893
22.300383	1114.861547	14.223911
22.165420	1109.135478	14.228928
22.153326	1107.017083	14.233946
22.186164	1131.092496	14.238963
22.324167	1118.261818	14.243981
22.008805	1120.187135	14.248999
22.230353	1125.243548	14.254016
22.557149	1120.203575	14.259034
22.288996	1128.955924	14.264051
22.601483	1130.905373	14.269069
22.423824	1116.408928	14.274087
22.293669	1092.379025	14.279104
22.155098	1090.895834	14.284122
22.035177	1132.166139	14.289139
22.305113	1107.984314	14.294157
22.187547	1127.320757	14.299175
22.592392	1136.253629	14.304192
22.549978	1138.446865	14.309210
22.305844	1136.518051	14.314227
22.480972	1128.653611	14.319245
22.360820	1137.217199	14.324263
22.131627	1122.445833	14.329280
22.257627	1133.922627	14.334298
22.374676	1141.820771	14.339315
22.503433	1112.390422	14.344333
22.022586	1134.875701	14.349351
22.501834	1140.042024	14.354368
22.516743	1158.226412	14.359386
22.775037	1160.255291	14.364403
22.602135	1148.345601	14.369421
22.745847	1164.820081	14.374439
23.021652	1161.131548	14.379456
23.046100	1155.068588	14.384474
22.684775	1159.293064	14.389491
22.984926	1166.466764	14.394509
22.838156	1167.610170	14.399527
22.771550	1161.155901	14.404544
22.842028	1163.708650	14.409562
22.846341	1157.543511	14.414579
22.926155	1153.296372	14.419597
22.521807	1176.183206	14.424615
22.565511	1155.636355	14.429632
22.573407	1183.221993	14.434650
21.879458	1166.184115	14.439667
22.979373	1156.545710	14.444685
22.544509	1170.573691	14.449703
22.768535	1207.383447	14.454720
23.026998	1187.120042	14.459738
23.366252	1184.020689	14.464755
23.124716	1213.660365	14.469773
23.265678	1169.411266	14.474791
23.576029	1205.208409	14.479808
23.284708	1192.741859	14.484826
23.030332	1163.476328	14.489843
23.108001	1200.433674	14.494861
23.663196	1165.220572	14.499879
23.396843	1172.467323	14.504896
23.243868	1158.525306	14.509914
23.117326	1168.197306	14.514931
23.513880	1140.723442	14.519949
22.856206	1174.010280	14.524967
23.215187	1148.367048	14.529984
23.612081	1187.716278	14.535002
23.420095	1150.849631	14.540019
23.508642	1168.877575	14.545037
23.177317	1164.375117	14.550055
23.239962	1144.514224	14.555072
23.598757	1148.538907	14.560090
23.356807	1151.869769	14.565107
23.360023	1153.489459	14.570125
23.329592	1192.620574	14.575143
23.589803	1210.113905	14.580160
23.679620	1177.242448	14.585178
23.437711	1216.016470	14.590195
23.911137	1189.608533	14.595213
23.481217	1204.710102	14.600231
23.759663	1162.741153	14.605248
23.592088	1191.732720	14.610266
23.566816	1210.805237	14.615283
23.507565	1189.534670	14.620301
24.164124	1190.515351	14.625319
23.881726	1208.603292	14.630336
23.497649	1166.490679	14.635354
23.248819	1150.860425	14.640371
23.525795	1199.271844	14.645389
23.884667	1176.244445	14.650407
23.422351	1222.067541	14.655424
23.504725	1196.801025	14.660442
23.549454	1189.393064	14.665459
23.814571	1162.721892	14.670477
23.854496	1177.286044	14.675495
23.680848	1205.684022	14.680512
24.145838	1163.899243	14.685530
23.922024	1219.331356	14.690547
24.042937	1190.768026	14.695565
24.035979	1178.418152	14.700583
23.882670	1205.384622	14.705600
23.719190	1187.768199	14.710618
23.882315	1178.502549	14.715635
23.936714	1213.988975	14.720653
23.913184	1209.607296	14.725671
23.889401	1199.486642	14.730688
24.035191	1231.180237	14.735706
24.236760	1213.865774	14.740723
24.280996	1247.610254	14.745741
24.106323	1221.240344	14.750759
24.742247	1197.170669	14.755776
24.434399	1237.901041	14.760794
24.055091	1205.700501	14.765811
24.326857	1195.892138	14.770829
24.382498	1233.170036	14.775847
24.510150	1184.602029	14.780864
24.343305	1207.589456	14.785882
23.952350	1197.932404	14.790899
24.707383	1189.292771	14.795917
24.391602	1200.413800	14.800935
23.877810	1227.503082	14.805952
24.455822	1207.922480	14.810970
24.565231	1201.688652	14.815987
24.693336	1236.914848	14.821005
24.837011	1198.353138	14.826023
24.469846	1234.680755	14.831040
25.078376	1184.780813	14.836058
24.616115	1213.373482	14.841075
24.281883	1194.905773	14.846093
24.827258	1164.784400	14.851111
24.569327	1199.670178	14.856128
24.601212	1177.442093	14.861146
24.859857	1197.310067	14.866163
24.424117	1202.861436	14.871181
24.808713	1167.798228	14.876199
24.762058	1194.782275	14.881216
24.613071	1183.364230	14.886234
24.776020	1159.675994	14.891251
24.557226	1186.687479	14.896269
24.960297	1224.029490	14.901287
24.348811	1216.708871	14.906304
24.848664	1200.462881	14.911322
25.243882	1201.955565	14.916339
25.036358	1229.030610	14.921357
25.281501	1182.428976	14.926375
24.826805	1221.597162	14.931392
25.370292	1175.971978	14.936410
24.995514	1201.795603	14.941427
25.244218	1182.855063	14.946445
25.134086	1179.906031	14.951463
25.318042	1158.671437	14.956480
25.301300	1189.306298	14.961498
24.926562	1196.704050	14.966515
24.587465	1190.504006	14.971533
24.932174	1175.472746	14.976551
25.083767	1165.318640	14.981568
25.081335	1201.206556	14.986586
24.969352	1212.081952	14.991603
24.934990	1197.176406	14.996621
25.470637	1179.347820	15.001639
25.083853	1196.424453	15.006656
25.328859	1232.062990	15.011674
25.839824	1200.211244	15.016691
25.367704	1220.473429	15.021709
25.445914	1177.030243	15.026727
24.931738	1208.369737	15.031744
25.121392	1173.604226	15.036762
25.375053	1215.718863	15.041779
25.129989	1224.986671	15.046797
25.988795	1185.233448	15.051815
25.666833	1231.427434	15.056832
25.081561	1226.012231	15.061850
25.416374	1206.387051	15.066867
25.263232	1189.020653	15.071885
25.352627	1191.071756	15.076903
24.736841	1244.134653	15.081920
25.352547	1224.992385	15.086938
25.184788	1202.836213	15.091955
25.552128	1229.429476	15.096973
26.015840	1265.501177	15.101991
25.853167	1249.106761	15.107008
25.965464	1207.889326	15.112026
25.846347	1249.161408	15.117043
25.651157	1229.387137	15.122061
25.812264	1198.695426	15.127079
25.866219	1200.572863	15.132096
25.723807	1233.064312	15.137114
25.757014	1236.993087	15.142131
25.511564	1213.786738	15.147149
26.413696	1187.977374	15.152167
26.006338	1226.428610	15.157184
26.186294	1234.519686	15.162202
26.110187	1217.971503	15.167219
26.421123	1179.430356	15.172237
26.374925	1183.681657	15.177255
26.056440	1184.201238	15.182272
26.048708	1186.492766	15.187290
26.192195	1226.576988	15.192307
25.710920	1234.996886	15.197325
25.738106	1223.561723	15.202343
25.473031	1220.294484	15.207360
25.737834	1197.778329	15.212378
26.048918	1185.948716	15.217395
25.694739	1235.654023	15.222413
26.284715	1259.176762	15.227431
26.082409	1270.997028	15.232448
26.206592	1236.258327	15.237466
26.473955	1252.717905	15.242483
26.304925	1231.261084	15.247501
26.406290	1264.153372	15.252519
25.910852	1249.954434	15.257536
26.466662	1241.986749	15.262554
26.232963	1246.275837	15.267571
26.497039	1224.863205	15.272589
26.411335	1271.830512	15.277607
26.041832	1243.129008	15.282624
26.659972	1212.961324	15.287642
26.317869	1252.939812	15.292659
26.234116	1230.833904	15.297677
26.418120	1253.606577	15.302695
26.383828	1242.267718	15.307712
26.187778	1255.628499	15.312730
26.587222	1249.500974	15.317747
26.411741	1295.364282	15.322765
26.641431	1259.935457	15.327783
26.942235	1248.991451	15.332800
26.892888	1288.622906	15.337818
27.036402	1253.981750	15.342835
27.137997	1252.243167	15.347853
26.871299	1279.591218	15.352871
26.378129	1253.382155	15.357888
26.761728	1217.390926	15.362906
26.894154	1233.831106	15.367923
26.989984	1281.231948	15.372941
27.065493	1287.184718	15.377959
26.722893	1269.142169	15.382976
26.546549	1263.664878	15.387994
27.519338	1248.350907	15.393011
27.625348	1227.680762	15.398029
27.246128	1222.267302	15.403047
27.063299	1222.941423	15.408064
26.910414	1261.503959	15.413082
26.533005	1238.658381	15.418099
27.361609	1218.967800	15.423117
27.158183	1232.483889	15.428135
26.921037	1245.665603	15.433152
26.704063	1238.080711	15.438170
27.089105	1234.185980	15.443187
26.831699	1270.718759	15.448205
27.248665	1291.919101	15.453223
27.047369	1305.880074	15.458240
27.060748	1296.998447	15.463258
27.476646	1273.290133	15.468275
27.202495	1294.789462	15.473293
27.460102	1286.855155	15.478311
27.661107	1263.056864	15.483328
27.438760	1246.469052	15.488346
27.505201	1274.731350	15.493363
27.464891	1300.670117	15.498381
27.667174	1285.955608	15.503399
27.479282	1289.402146	15.508416
27.583075	1300.251846	15.513434
27.510858	1287.602407	15.518451
27.437316	1263.493979	15.523469
27.961302	1235.187952	15.528487
27.434734	1237.537068	15.533504
27.517326	1246.225683	15.538522
27.649562	1269.077421	15.543539
27.480315	1290.800681	15.548557
27.005837	1272.997805	15.553575
26.645670	1275.450946	15.558592
27.593606	1274.532184	15.563610
28.287399	1269.329812	15.568627
28.005715	1270.405082	15.573645
28.169142	1297.423453	15.578663
27.684153	1316.357860	15.583680
27.711911	1306.504971	15.588698
27.797241	1298.801049	15.593715
28.013053	1280.730772	15.598733
27.860695	1324.614812	15.603751
27.814048	1313.628646	15.608768
27.777234	1273.051420	15.613786
28.103588	1291.964934	15.618803
27.999046	1331.967097	15.623821
27.965792	1301.912556	15.628839
27.833476	1290.941643	15.633856
27.961839	1274.359212	15.638874
28.447022	1310.971857	15.643891
28.121327	1284.451315	15.648909
28.173695	1283.837401	15.653927
28.203744	1296.226232	15.658944
28.131938	1309.891283	15.663962
28.499535	1276.112514	15.668979
28.015828	1318.814587	15.673997
28.184284	1308.827574	15.679015
28.446976	1273.599514	15.684032
28.397149	1262.533671	15.689050
28.399901	1294.241567	15.694067
28.028331	1298.049301	15.699085
28.343086	1291.685160	15.704103
28.127418	1301.708082	15.709120
28.383838	1283.329312	15.714138
28.845160	1320.590711	15.719155
28.782087	1295.310254	15.724173
28.688359	1298.111007	15.729191
28.727593	1280.666629	15.734208
28.382937	1293.893846	15.739226
29.106564	1282.676319	15.744243
28.751882	1278.034408	15.749261
28.643489	1284.689746	15.754279
28.822402	1266.205384	15.759296
28.687612	1293.266590	15.764314
28.989693	1262.029243	15.769331
28.528367	1302.651357	15.774349
28.831710	1265.828112	15.779367
28.784327	1295.137336	15.784384
29.007206	1263.912617	15.789402
29.168273	1300.630409	15.794419
28.936311	1272.893174	15.799437
28.793869	1290.733172	15.804455
28.859788	1285.505093	15.809472
29.094519	1277.951956	15.814490
29.149309	1274.893233	15.819507
29.022492	1294.769336	15.824525
29.030946	1272.535404	15.829543
29.190269	1294.753667	15.834560
28.940687	1275.349795	15.839578
29.069609	1289.755152	15.844595
28.938661	1280.383758	15.849613
28.770328	1277.456572	15.854631
28.992931	1310.318619	15.859648
28.927659	1309.185503	15.864666
29.661867	1294.183235	15.869683
29.076968	1322.458271	15.874701
29.519979	1304.207016	15.879719
29.571667	1315.643898	15.884736
29.325036	1315.028906	15.889754
29.815665	1310.338685	15.894771
29.680173	1305.402264	15.899789
29.508065	1305.744350	15.904807
29.206852	1288.654700	15.909824
29.188438	1319.373470	15.914842
29.670967	1293.895890	15.919859
29.896908	1292.316791	15.924877
29.544295	1333.513098	15.929895
29.949731	1280.364739	15.934912
29.509318	1307.663472	15.939930
29.317110	1288.259871	15.944947
29.627845	1285.542562	15.949965
29.512565	1333.241506	15.954983
29.139737	1310.788332	15.960000
29.599601	1309.856175	15.965018
30.007009	1307.595343	15.970035
29.753897	1309.452555	15.975053
29.700283	1306.573132	15.980071
29.790344	1280.684698	15.985088
29.740348	1318.848741	15.990106
29.841468	1303.142061	15.995123
29.470800	1306.800219	16.000141
29.641094	1295.255661	16.005159
29.927139	1316.480067	16.010176
29.460238	1305.549920	16.015194
30.251700	1322.572491	16.020211
29.972090	1370.700453	16.025229
30.122889	1331.147051	16.030247
30.239678	1345.571701	16.035264
30.003230	1341.771342	16.040282
30.513575	1304.763976	16.045299
30.330145	1319.809050	16.050317
30.403303	1351.365846	16.055335
30.295973	1324.574455	16.060352
29.894764	1310.837045	16.065370
30.548066	1297.211461	16.070387
30.905000	1293.066374	16.075405
30.365501	1328.458254	16.080423
30.172517	1301.656970	16.085440
30.295455	1274.931191	16.090458
30.330722	1300.230282	16.095475
30.537494	1335.042273	16.100493
30.371290	1309.295330	16.105511
30.844279	1294.605277	16.110528
30.511356	1357.390960	16.115546
30.453862	1322.432493	16.120563
30.828609	1287.625392	16.125581
30.518136	1335.986245	16.130599
30.918560	1294.109144	16.135616
30.546849	1332.403182	16.140634
30.652281	1308.937802	16.145651
30.593416	1323.808861	16.150669
30.987638	1302.348618	16.155687
31.128079	1343.384522	16.160704
30.656035	1313.303985	16.165722
30.809849	1287.548513	16.170739
30.767702	1327.290608	16.175757
31.010459	1322.274980	16.180775
31.049515	1318.567539	16.185792
30.830643	1338.335689	16.190810
31.008556	1304.230037	16.195827
30.985595	1347.959807	16.200845
30.766196	1315.877446	16.205863
31.140754	1324.212811	16.210880
30.622712	1336.887285	16.215898
30.995187	1300.625496	16.220915
31.008950	1343.813008	16.225933
30.541581	1326.238588	16.230951
31.147472	1288.948616	16.235968
30.765058	1337.336677	16.240986
31.019658	1318.050535	16.246003
30.813345	1327.360990	16.251021
30.724280	1345.134341	16.256039
31.329551	1350.414348	16.261056
31.201386	1344.169586	16.266074
31.105252	1353.062945	16.271091
31.416624	1354.284306	16.276109
31.141205	1347.081477	16.281127
31.875919	1336.230222	16.286144
31.427980	1360.228539	16.291162
31.680387	1330.798476	16.296179
31.252367	1360.126066	16.301197
31.430909	1337.311213	16.306215
31.314240	1351.604792	16.311232
31.589078	1321.247822	16.316250
31.499839	1316.020882	16.321267
31.412299	1358.419221	16.326285
31.292697	1366.136583	16.331303
31.768707	1361.568225	16.336320
32.088987	1386.027647	16.341338
31.762224	1362.336960	16.346355
31.983766	1389.467355	16.351373
31.577723	1365.904134	16.356391
31.986769	1386.884088	16.361408
31.795820	1350.872477	16.366426
31.862686	1393.189664	16.371443
31.984446	1371.923780	16.376461
32.290033	1351.303425	16.381479
32.531589	1372.599502	16.386496
32.422114	1395.582795	16.391514
32.180397	1337.313504	16.396531
31.884845	1354.490600	16.401549
32.424139	1332.404718	16.406567
31.867572	1347.119227	16.411584
32.177955	1352.290539	16.416602
32.234129	1350.810867	16.421619
32.438987	1373.835229	16.426637
32.198807	1354.868617	16.431655
31.983553	1365.478245	16.436672
32.470018	1356.091703	16.441690
32.352139	1370.992671	16.446707
32.683080	1365.833979	16.451725
32.137477	1372.505603	16.456743
32.760906	1361.303996	16.461760
32.785312	1377.346296	16.466778
32.388808	1365.039513	16.471795
32.505447	1344.186611	16.476813
32.521841	1355.226467	16.481831
32.710542	1374.571023	16.486848
32.767360	1353.748097	16.491866
32.988934	1367.364841	16.496883
32.555229	1353.873240	16.501901
32.410260	1331.456050	16.506919
32.568308	1359.287060	16.511936
32.693265	1358.891224	16.516954
32.346072	1373.498437	16.521971
33.078331	1368.826289	16.526989
32.757691	1361.566172	16.532007
32.586598	1377.505946	16.537024
32.939472	1366.053335	16.542042
32.677685	1355.334251	16.547059
33.062759	1383.251794	16.552077
32.611337	1369.667051	16.557095
33.236179	1348.981626	16.562112
33.099654	1379.889246	16.567130
32.786433	1368.734769	16.572147
32.916323	1363.313992	16.577165
32.860702	1386.736987	16.582183
32.656041	1375.173515	16.587200
33.262923	1359.661387	16.592218
32.991517	1405.145520	16.597235
33.262910	1393.480942	16.602253
33.159914	1369.913428	16.607271
33.393762	1421.258246	16.612288
33.285681	1387.028126	16.617306
33.225628	1412.268684	16.622323
33.342878	1380.695624	16.627341
33.240147	1404.480086	16.632359
33.192131	1375.974006	16.637376
32.869059	1403.008815	16.642394
33.576672	1379.359196	16.647411
33.482753	1404.485594	16.652429
33.202679	1379.840484	16.657447
33.430312	1430.807234	16.662464
33.395843	1417.283363	16.667482
33.695334	1432.841412	16.672499
33.743580	1417.660559	16.677517
33.943814	1440.349141	16.682535
33.703976	1414.736448	16.687552
33.812295	1427.306387	16.692570
33.883497	1438.567224	16.697587
34.262232	1398.955263	16.702605
33.897808	1390.687529	16.707623
34.087202	1429.799956	16.712640
34.214247	1439.711688	16.717658
34.014899	1390.708296	16.722675
34.143523	1409.247665	16.727693
34.199505	1411.731985	16.732711
33.695430	1386.084407	16.737728
34.196496	1379.075471	16.742746
33.973279	1427.458891	16.747763
34.037602	1444.243649	16.752781
33.968366	1451.561346	16.757799
34.109867	1430.998507	16.762816
33.948285	1422.729864	16.767834
34.490795	1395.782793	16.772851
34.422030	1431.774667	16.777869
34.223367	1450.300219	16.782887
34.055840	1415.530533	16.787904
34.645458	1390.675918	16.792922
34.507378	1411.692830	16.797939
34.559487	1443.311384	16.802957
33.993679	1434.054861	16.807975
34.603630	1394.310084	16.812992
35.031694	1433.017948	16.818010
34.454173	1454.976450	16.823027
34.462899	1431.104731	16.828045
34.479642	1415.903736	16.833063
34.534858	1392.611395	16.838080
34.415102	1438.516606	16.843098
34.666469	1402.097702	16.848115
34.579000	1432.143469	16.853133
34.454168	1404.925290	16.858151
34.720708	1454.495385	16.863168
34.482158	1441.622231	16.868186
35.231384	1428.402794	16.873203
35.261224	1406.825906	16.878221
35.270442	1445.882171	16.883239
35.323177	1447.165238	16.888256
34.987932	1411.822993	16.893274
34.740474	1402.650997	16.898291
34.865954	1424.730141	16.903309
35.206879	1421.595867	16.908327
35.140849	1446.094980	16.913344
35.178721	1431.939793	16.918362
35.109695	1429.143027	16.923379
35.346460	1460.156449	16.928397
35.403023	1432.374466	16.933415
35.139251	1460.164405	16.938432
34.955783	1442.198505	16.943450
35.218240	1426.937862	16.948467
35.792983	1457.688167	16.953485
35.141432	1455.893498	16.958503
35.456353	1422.365033	16.963520
35.732400	1459.981954	16.968538
35.307906	1458.234441	16.973555
35.675801	1431.379646	16.978573
35.439610	1450.439713	16.983591
35.790179	1414.327423	16.988608
35.695429	1461.526447	16.993626
35.533080	1456.864814	16.998643
35.920467	1434.762106	17.003661
35.610359	1437.248188	17.008679
35.849156	1424.777113	17.013696
35.641516	1455.678932	17.018714
35.230916	1468.388294	17.023731
35.822425	1457.819335	17.028749
35.469298	1448.344842	17.033767
35.932527	1435.001126	17.038784
35.907326	1458.861400	17.043802
35.948955	1456.157092	17.048819
35.938376	1478.678011	17.053837
36.357491	1458.709500	17.058855
36.129388	1471.635149	17.063872
36.395294	1431.559753	17.068890
35.937609	1462.956064	17.073907
35.815957	1465.201311	17.078925
36.223309	1442.238118	17.083943
36.313978	1479.106015	17.088960
36.532943	1455.052863	17.093978
36.168451	1478.714027	17.098995
36.679221	1461.913094	17.104013
36.381326	1459.360460	17.109031
36.869093	1445.577098	17.114048
36.673563	1450.780367	17.119066
36.024990	1433.447071	17.124083
36.374848	1410.658262	17.129101
36.391367	1466.815113	17.134119
36.444514	1447.883394	17.139136
36.750096	1470.141522	17.144154
36.825116	1442.559494	17.149171
36.890342	1470.223052	17.154189
36.798846	1458.613151	17.159207
36.765523	1454.371384	17.164224
36.640160	1454.893205	17.169242
37.013854	1435.175787	17.174259
36.814784	1415.131322	17.179277
36.573311	1467.904895	17.184295
36.697458	1478.537554	17.189312
36.497125	1460.407582	17.194330
37.119154	1441.562894	17.199347
37.117909	1485.451636	17.204365
37.090602	1448.830096	17.209383
37.270361	1425.406156	17.214400
37.453069	1459.964314	17.219418
37.369142	1480.967971	17.224435
36.811478	1461.803315	17.229453
37.293846	1441.508566	17.234471
37.112382	1441.317324	17.239488
37.111941	1469.294943	17.244506
36.624518	1490.642960	17.249523
36.856792	1486.833875	17.254541
36.778867	1468.130671	17.259559
36.662283	1472.493954	17.264576
37.490252	1450.188825	17.269594
37.185526	1510.636332	17.274611
37.171843	1486.433043	17.279629
37.619277	1466.417535	17.284647
37.549661	1512.267792	17.289664
37.951005	1471.476987	17.294682
37.758196	1500.718585	17.299699
38.218302	1456.608832	17.304717
38.133096	1480.772865	17.309735
37.807127	1517.078101	17.314752
37.535257	1472.641447	17.319770
37.680214	1463.990414	17.324787
37.350388	1503.693930	17.329805
37.353384	1471.361826	17.334823
37.529629	1503.467223	17.339840
37.700603	1478.661921	17.344858
37.891161	1534.388586	17.349875
37.877975	1499.634982	17.354893
38.422780	1529.235624	17.359911
38.183259	1499.455813	17.364928
38.344887	1516.975463	17.369946
38.531634	1502.558940	17.374963
38.311374	1510.943659	17.379981
38.392884	1468.629283	17.384999
37.865615	1490.343873	17.390016
38.333626	1461.196909	17.395034
37.930484	1490.756746	17.400051
38.403391	1517.864597	17.405069
38.733118	1499.873408	17.410087
38.420220	1517.597725	17.415104
38.696132	1510.124417	17.420122
38.864869	1472.792009	17.425139
38.544923	1495.071285	17.430157
38.660897	1456.866446	17.435175
38.431118	1469.877303	17.440192
38.440706	1476.535934	17.445210
38.301121	1469.215427	17.450227
38.893078	1502.069342	17.455245
38.742106	1493.633799	17.460263
38.642311	1508.066412	17.465280
38.467592	1506.224003	17.470298
38.925588	1473.885395	17.475315
38.768314	1526.427104	17.480333
38.689947	1498.597300	17.485351
38.716102	1516.888883	17.490368
38.674105	1508.646736	17.495386
38.941737	1510.046546	17.500403
38.598032	1508.323895	17.505421
39.047062	1529.980369	17.510439
39.079225	1517.128466	17.515456
39.365963	1538.560726	17.520474
39.596218	1525.571832	17.525491
39.293379	1510.909340	17.530509
39.373511	1523.337568	17.535527
39.020731	1524.342396	17.540544
39.180994	1504.748584	17.545562
39.393014	1507.143542	17.550579
39.328011	1544.778895	17.555597
39.456660	1506.962011	17.560615
39.305501	1549.013980	17.565632
39.326700	1529.508379	17.570650
40.049068	1494.576132	17.575667
40.031899	1533.204262	17.580685
39.775269	1523.220402	17.585703
39.694551	1543.032864	17.590720
40.120058	1514.620879	17.595738
39.625082	1508.212750	17.600755
39.805350	1504.839814	17.605773
39.918990	1488.541056	17.610791
39.838645	1507.787127	17.615808
39.949949	1485.231301	17.620826
39.710213	1492.508570	17.625843
39.726806	1506.921047	17.630861
39.808962	1510.160975	17.635879
39.783112	1522.760260	17.640896
39.941820	1527.564144	17.645914
39.705185	1536.264519	17.650931
39.686022	1533.832586	17.655949
39.954828	1515.088181	17.660967
39.463336	1541.362028	17.665984
39.984002	1551.218926	17.671002
40.127646	1539.664268	17.676019
40.281555	1548.066413	17.681037
40.481695	1562.342708	17.686055
40.385496	1549.283160	17.691072
40.330067	1560.166314	17.696090
40.384005	1555.956218	17.701107
40.062792	1574.027994	17.706125
40.348491	1539.484603	17.711143
40.357325	1560.756724	17.716160
40.387841	1543.055445	17.721178
40.269526	1545.136578	17.726195
40.521164	1563.426866	17.731213
40.990397	1575.300730	17.736231
40.811509	1569.973164	17.741248
40.747618	1555.717683	17.746266
40.838759	1564.936807	17.751283
40.553111	1575.650622	17.756301
41.141008	1588.959043	17.761319
41.012598	1576.947522	17.766336
41.448725	1580.206519	17.771354
41.187875	1557.019376	17.776371
41.307728	1549.676329	17.781389
41.282785	1553.551543	17.786407
41.222219	1540.380929	17.791424
41.202105	1543.063023	17.796442
41.276984	1532.840671	17.801459
40.856480	1547.060203	17.806477
41.029663	1549.527428	17.811495
40.977733	1535.517022	17.816512
41.132119	1575.034973	17.821530
41.230842	1560.522319	17.826547
41.400410	1586.833966	17.831565
41.509263	1555.747927	17.836583
41.641119	1598.791523	17.841600
41.650339	1547.232783	17.846618
41.889662	1584.185778	17.851635
41.262380	1557.818223	17.856653
41.269146	1572.427386	17.861671
41.717615	1545.966942	17.866688
41.731566	1581.527573	17.871706
42.018423	1564.828299	17.876723
41.442867	1584.987149	17.881741
41.715298	1552.184033	17.886759
41.564358	1593.901044	17.891776
41.451359	1557.313345	17.896794
41.708513	1594.189590	17.901811
41.957471	1570.011915	17.906829
42.448737	1607.286584	17.911847
42.180408	1597.878692	17.916864
42.142533	1569.918025	17.921882
42.316622	1607.751364	17.926899
42.133202	1583.571836	17.931917
42.375921	1548.033265	17.936935
42.016131	1584.137997	17.941952
42.557480	1551.652216	17.946970
42.684132	1584.214012	17.951987
42.218048	1556.057394	17.957005
42.245394	1572.546179	17.962023
42.182817	1553.849854	17.967040
42.177841	1594.821574	17.972058
42.836723	1591.202403	17.977075
42.030489	1599.633433	17.982093
42.572612	1594.140535	17.987111
42.342558	1602.659003	17.992128
42.468240	1581.585668	17.997146
42.773948	1608.574065	18.002163
42.628242	1583.581562	18.007181
42.624729	1592.947933	18.012199
42.617748	1584.303757	18.017216
42.331401	1608.316036	18.022234
42.911772	1597.526959	18.027251
42.833135	1631.328108	18.032269
43.243038	1591.060994	18.037287
43.199739	1632.545445	18.042304
43.130519	1644.730181	18.047322
43.318056	1615.657526	18.052339
43.327539	1609.006878	18.057357
43.648530	1576.106301	18.062375
43.141966	1577.437678	18.067392
43.105997	1611.489953	18.072410
43.658969	1583.441323	18.077427
43.756636	1596.247488	18.082445
43.623327	1585.531338	18.087463
43.428850	1568.306356	18.092480
43.607150	1594.863590	18.097498
43.858900	1562.787338	18.102515
43.581941	1588.492229	18.107533
43.731728	1555.389341	18.112551
43.397921	1583.958319	18.117568
43.327780	1568.149677	18.122586
43.438056	1560.625681	18.127603
43.383856	1592.911173	18.132621
43.790877	1591.300020	18.137639
43.565579	1599.957727	18.142656
43.657896	1607.397601	18.147674
43.799193	1588.384001	18.152691
43.548349	1614.929487	18.157709
43.908914	1606.561736	18.162727
43.916165	1595.945858	18.167744
44.021487	1598.376723	18.172762
43.953414	1611.272255	18.177779
43.808913	1595.472296	18.182797
43.874729	1610.002867	18.187815
44.145541	1605.375925	18.192832
44.054578	1660.300113	18.197850
44.414692	1618.330980	18.202867
44.550353	1639.696249	18.207885
44.462584	1628.552806	18.212903
44.277726	1643.285410	18.217920
44.403679	1623.029946	18.222938
44.385257	1653.760438	18.227955
44.168819	1618.378291	18.232973
44.494800	1609.758077	18.237991
44.554418	1656.947275	18.243008
44.107158	1639.443198	18.248026
45.093612	1607.295295	18.253043
44.699143	1632.256088	18.258061
44.682328	1648.308408	18.263079
44.302912	1630.870599	18.268096
44.730211	1634.052365	18.273114
44.542373	1661.871479	18.278131
44.853223	1643.115485	18.283149
44.859275	1674.726160	18.288167
44.717253	1646.596336	18.293184
44.939486	1673.941087	18.298202
45.456302	1650.480335	18.303219
45.031962	1650.898833	18.308237
44.914719	1669.718420	18.313255
45.335266	1653.744913	18.318272
45.232891	1670.855395	18.323290
45.464682	1658.002992	18.328307
45.257013	1653.416163	18.333325
45.488363	1658.376820	18.338343
45.633681	1654.090775	18.343360
45.594855	1647.161523	18.348378
45.678015	1656.234113	18.353395
45.480442	1651.043205	18.358413
45.447270	1671.059045	18.363431
45.653456	1650.471423	18.368448
45.856168	1673.108066	18.373466
45.677110	1671.702057	18.378483
45.765476	1656.967588	18.383501
45.586473	1688.541738	18.388519
46.325899	1664.549956	18.393536
45.895628	1686.197457	18.398554
46.337412	1672.339418	18.403571
46.383325	1661.923393	18.408589
46.110250	1656.019357	18.413607
45.923635	1648.918618	18.418624
45.942304	1650.391180	18.423642
45.987788	1661.443934	18.428659
46.006433	1673.974906	18.433677
46.338346	1675.966952	18.438695
46.595851	1692.733774	18.443712
46.146166	1670.320610	18.448730
46.408930	1671.771550	18.453747
46.298057	1688.285655	18.458765
46.189398	1673.278995	18.463783
46.467594	1674.615790	18.468800
46.403204	1694.174169	18.473818
46.733399	1663.258668	18.478835
46.268113	1679.176477	18.483853
46.558396	1692.814031	18.488871
46.546019	1653.158359	18.493888
46.374325	1698.147733	18.498906
46.790966	1666.055968	18.503923
46.560647	1685.986866	18.508941
46.905054	1682.520072	18.513959
47.004691	1681.322874	18.518976
46.995817	1700.037129	18.523994
47.456012	1699.924451	18.529011
47.264663	1699.994332	18.534029
46.826827	1684.115213	18.539047
47.217778	1683.603017	18.544064
47.080030	1697.975803	18.549082
47.037338	1696.905123	18.554099
47.492159	1700.035324	18.559117
47.051099	1708.634696	18.564135
47.599526	1699.742999	18.569152
47.586146	1690.995959	18.574170
47.595067	1698.667833	18.579187
47.316161	1707.717973	18.584205
47.258164	1688.199620	18.589223
47.295059	1708.592877	18.594240
47.211430	1693.623104	18.599258
47.362128	1677.514853	18.604275
47.511284	1720.073131	18.609293
47.667298	1706.930747	18.614311
47.477285	1734.364952	18.619328
47.820168	1707.496333	18.624346
47.705388	1728.703471	18.629363
47.475761	1715.743704	18.634381
47.577034	1739.008538	18.639399
48.002095	1703.962755	18.644416
47.983782	1716.159882	18.649434
48.152298	1750.205040	18.654451
48.046256	1732.456094	18.659469
47.810829	1733.181096	18.664487
48.745394	1728.262644	18.669504
48.441603	1710.109530	18.674522
48.646225	1726.186398	18.679539
48.389094	1747.549973	18.684557
48.171599	1724.778794	18.689575
48.969874	1714.510163	18.694592
48.667250	1731.325459	18.699610
48.557533	1711.796446	18.704627
48.536490	1746.499467	18.709645
48.029322	1747.494324	18.714663
48.649463	1753.634138	18.719680
48.236900	1750.888950	18.724698
48.535011	1740.426356	18.729715
49.002888	1726.232194	18.734733
48.651332	1719.220646	18.739751
48.818627	1764.912796	18.744768
48.624574	1745.809325	18.749786
49.279281	1708.153416	18.754803
49.210464	1750.337555	18.759821
49.844192	1715.082287	18.764839
49.723281	1745.577632	18.769856
49.209421	1765.275429	18.774874
49.580444	1725.166728	18.779891
49.348933	1755.467373	18.784909
49.489470	1743.736867	18.789927
49.104648	1739.367028	18.794944
49.621970	1729.858923	18.799962
49.667494	1767.793409	18.804979
49.351948	1739.282088	18.809997
49.618864	1708.735234	18.815015
49.458952	1750.562666	18.820032
49.216308	1754.872204	18.825050
49.626255	1718.241599	18.830067
49.344566	1724.152413	18.835085
49.531451	1758.534437	18.840103
49.673366	1716.549481	18.845120
49.496603	1760.641655	18.850138
49.893597	1743.638319	18.855155
49.902889	1785.037740	18.860173
49.620339	1784.905085	18.865191
49.840794	1762.299961	18.870208
49.908887	1768.488496	18.875226
49.924968	1797.151531	18.880243
49.956656	1774.002332	18.885261
50.175492	1748.952980	18.890279
50.188512	1767.558436	18.895296
50.176889	1773.292492	18.900314
50.482987	1761.757368	18.905331
50.596071	1808.767072	18.910349
50.400462	1780.994749	18.915367
50.767582	1785.992001	18.920384
50.633850	1819.991142	18.925402
50.588875	1800.333707	18.930419
50.556994	1770.635055	18.935437
50.627231	1773.574919	18.940455
50.682065	1792.505650	18.945472
50.661640	1821.374332	18.950490
50.342813	1813.750322	18.955507
50.666248	1795.539546	18.960525
50.396747	1790.328597	18.965543
50.981269	1780.652439	18.970560
50.720668	1806.042070	18.975578
51.226968	1842.633820	18.980595
51.479590	1798.236793	18.985613
51.521560	1797.470358	18.990631
51.923559	1828.000463	18.995648
51.688548	1802.369009	19.000666
51.543567	1782.383049	19.005683
52.188438	1751.078974	19.010701
51.598445	1790.596673	19.015719
51.822881	1759.515361	19.020736
51.881727	1768.694147	19.025754
51.679244	1775.827188	19.030771
51.938941	1729.283612	19.035789
51.276627	1779.185425	19.040807
51.523872	1763.753821	19.045824
51.836425	1744.890458	19.050842
51.482210	1777.409825	19.055859
51.775747	1786.134339	19.060877
51.914415	1753.971878	19.065895
52.247071	1727.918114	19.070912
51.960172	1731.918522	19.075930
51.866955	1763.312412	19.080947
52.207422	1790.328640	19.085965
51.787498	1771.777113	19.090983
52.441981	1747.956046	19.096000
52.469850	1724.469330	19.101018
52.160805	1737.530819	19.106035
52.086337	1763.784179	19.111053
52.253251	1759.851739	19.116071
52.071556	1786.921345	19.121088
51.918802	1794.631637	19.126106
51.945047	1789.526109	19.131123
52.657243	1766.433566	19.136141
52.279546	1823.507255	19.141159
52.382556	1790.263425	19.146176
52.245562	1812.059399	19.151194
52.427701	1803.428978	19.156211
52.810367	1822.842303	19.161229
53.093084	1829.595968	19.166247
53.203698	1821.571554	19.171264
52.842248	1838.105341	19.176282
52.688345	1859.801835	19.181299
53.018831	1818.670566	19.186317
52.864121	1846.487896	19.191335
52.878238	1819.345880	19.196352
52.816076	1836.750595	19.201370
52.973220	1839.050540	19.206387
52.729838	1845.693054	19.211405
53.104415	1841.850173	19.216423
52.979067	1864.367971	19.221440
53.397042	1859.676581	19.226458
53.139419	1873.200334	19.231475
53.958418	1827.902769	19.236493
53.648164	1857.487863	19.241511
53.775298	1869.743722	19.246528
53.477379	1861.045104	19.251546
53.954811	1825.053138	19.256563
54.137237	1827.013990	19.261581
53.760563	1887.428920	19.266599
53.866139	1879.690001	19.271616
53.841882	1866.604537	19.276634
53.812703	1846.279119	19.281651
54.310751	1870.899781	19.286669
54.034483	1860.011167	19.291687
54.307834	1830.749788	19.296704
54.204394	1862.933620	19.301722
54.040520	1850.751345	19.306739
54.437127	1852.723662	19.311757
54.687018	1862.682162	19.316775
54.654019	1871.413183	19.321792
54.853701	1823.961786	19.326810
54.195182	1860.745636	19.331827
54.703112	1826.309270	19.336845
54.470003	1866.366445	19.341863
54.263695	1843.774196	19.346880
54.662208	1863.678987	19.351898
54.527667	1874.405103	19.356915
54.820130	1863.949614	19.361933
54.713305	1865.747384	19.366951
54.958771	1881.187116	19.371968
54.932674	1883.134038	19.376986
54.462491	1863.566350	19.382003
54.888790	1847.495759	19.387021
54.722678	1884.013947	19.392039
54.848815	1884.313201	19.397056
55.401386	1877.764587	19.402074
55.768731	1865.296232	19.407091
55.822899	1906.059622	19.412109
55.253024	1874.657989	19.417127
55.922485	1858.784565	19.422144
55.682200	1879.094848	19.427162
55.643340	1856.293401	19.432179
55.620430	1873.006050	19.437197
55.802674	1837.279784	19.442215
55.864941	1885.367515	19.447232
55.674136	1861.323983	19.452250
55.738209	1860.137161	19.457267
55.743875	1866.618843	19.462285
55.467041	1870.052957	19.467303
56.211701	1860.259973	19.472320
56.647496	1866.548789	19.477338
56.117881	1908.854066	19.482355
55.758419	1877.050776	19.487373
55.926634	1866.256444	19.492391
55.808155	1897.958253	19.497408
55.980674	1902.686126	19.502426
56.178458	1875.256734	19.507443
56.138994	1886.434893	19.512461
55.872920	1916.428347	19.517479
56.293905	1898.618746	19.522496
56.429182	1923.034649	19.527514
56.377659	1916.969328	19.532531
56.658079	1924.766341	19.537549
56.997499	1901.953261	19.542567
56.634981	1940.909690	19.547584
56.880137	1893.142496	19.552602
56.679137	1927.407450	19.557619
56.661055	1925.783831	19.562637
56.766499	1888.856858	19.567655
56.799809	1939.179975	19.572672
56.905068	1911.106159	19.577690
56.803207	1910.279284	19.582707
56.733753	1931.380386	19.587725
57.300028	1933.473525	19.592743
57.553035	1959.539731	19.597760
57.805808	1928.401628	19.602778
57.526519	1936.772409	19.607795
57.873182	1933.607226	19.612813
57.745294	1908.531093	19.617831
57.097152	1923.446402	19.622848
57.730540	1901.009596	19.627866
57.407264	1930.716467	19.632883
57.935279	1908.729044	19.637901
58.076397	1951.242092	19.642919
57.884748	1910.102594	19.647936
57.903216	1932.702958	19.652954
57.437680	1920.774801	19.657971
58.199238	1930.706808	19.662989
57.806652	1940.511412	19.668007
58.101258	1925.594340	19.673024
58.398011	1933.143356	19.678042
58.004524	1935.737198	19.683059
58.097958	1926.806238	19.688077
58.126164	1944.449934	19.693095
57.986061	1914.612512	19.698112
58.392064	1931.758634	19.703130
58.184435	1927.078900	19.708147
58.170608	1954.521604	19.713165
58.383699	1936.971631	19.718183
58.568797	1964.285100	19.723200
58.958658	1936.085623	19.728218
58.498810	1966.968973	19.733235
58.926856	1954.394905	19.738253
58.845886	1951.304207	19.743271
58.845294	1946.448301	19.748288
58.854263	1968.745062	19.753306
58.753819	1952.297450	19.758323
58.894836	1936.179446	19.763341
58.621463	1955.180034	19.768359
58.345493	1979.340711	19.773376
59.347212	1973.212798	19.778394
59.344399	1988.866849	19.783411
59.454088	1995.723693	19.788429
59.532239	1973.208577	19.793447
59.122786	1973.045818	19.798464
59.517906	1980.969292	19.803482
59.460783	1961.341891	19.808499
59.465090	1990.702480	19.813517
59.243965	1964.829418	19.818535
59.618447	2017.494173	19.823552
60.159869	1986.229689	19.828570
59.815751	2011.991656	19.833587
60.174533	1995.370085	19.838605
60.168196	1974.724658	19.843623
59.963619	1988.685235	19.848640
60.163291	1953.504904	19.853658
60.338757	1999.091095	19.858675
60.301680	1967.459570	19.863693
60.490111	1975.032175	19.868711
60.777704	1949.929039	19.873728
60.952330	1979.643126	19.878746
60.572620	1944.205993	19.883763
60.570283	1978.735123	19.888781
61.059246	1943.680145	19.893799
60.978990	1981.146027	19.898816
60.788380	1948.223946	19.903834
60.482539	1975.996410	19.908851
60.879650	1947.842945	19.913869
60.372863	1977.579177	19.918887
60.540116	1949.880800	19.923904
60.788829	1978.788674	19.928922
60.646662	1939.826187	19.933939
60.595149	1976.606338	19.938957
60.777192	1958.340827	19.943975
60.797406	1997.892340	19.948992
60.963423	1976.966160	19.954010
61.004292	2012.164897	19.959027
61.010570	2006.697525	19.964045
61.337514	1997.905467	19.969063
60.781801	1997.670075	19.974080
61.557398	1992.485874	19.979098
61.366008	2041.574144	19.984115
61.509109	2008.829949	19.989133
61.944259	1992.855318	19.994151
61.662328	2016.239912	19.999168
61.649831	2047.791435	20.004186
61.366342	2038.020718	20.009203
62.001609	2010.318380	20.014221
61.902782	2031.831737	20.019239
61.977181	2011.330690	20.024256
62.157294	2033.957344	20.029274
62.175192	2007.210788	20.034291
62.305014	2023.981054	20.039309
62.379828	2050.613830	20.044327
62.414904	2019.884640	20.049344
62.496553	2058.207391	20.054362
62.198239	2017.007520	20.059379
62.364335	2048.626521	20.064397
62.666547	2005.054682	20.069415
62.224957	2062.142642	20.074432
62.687193	2044.323139	20.079450
62.622317	2030.315893	20.084467
62.709771	2013.303403	20.089485
62.962961	2052.581952	20.094503
62.492231	2042.370743	20.099520
63.324005	1997.399389	20.104538
63.063726	2033.288013	20.109555
62.969732	2042.579438	20.114573
63.092692	2007.286938	20.119591
63.431102	1999.501386	20.124608
63.708927	2025.950730	20.129626
63.706051	2025.779763	20.134643
63.262877	1994.632948	20.139661
63.641260	1994.866809	20.144679
62.960951	2027.858746	20.149696
63.398196	2022.188931	20.154714
63.981320	2002.470384	20.159731
63.728874	1989.748395	20.164749
63.629040	2010.336919	20.169767
63.261129	2057.437507	20.174784
63.482679	2072.397538	20.179802
63.945764	2066.768417	20.184819
63.393304	2046.890333	20.189837
64.001656	2033.038426	20.194855
63.986212	2051.910702	20.199872
63.927979	2073.153371	20.204890
63.968244	2055.380697	20.209907
64.585621	2043.780767	20.214925
64.256007	2029.178646	20.219943
64.113532	2083.755564	20.224960
64.296452	2098.459865	20.229978
64.416887	2106.187319	20.234995
64.232477	2094.480822	20.240013
64.749590	2043.737549	20.245031
64.802980	2094.260929	20.250048
64.495024	2061.538995	20.255066
64.712636	2093.491236	20.260083
64.926939	2052.075805	20.265101
65.197272	2045.789998	20.270119
64.824010	2077.721598	20.275136
64.941174	2051.214754	20.280154
65.386499	2040.660042	20.285171
65.215385	2087.188993	20.290189
65.517436	2058.566753	20.295207
65.638091	2054.939709	20.300224
65.685118	2071.013778	20.305242
65.806527	2038.074769	20.310259
65.567276	2044.545248	20.315277
65.643552	2075.090853	20.320295
65.458283	2043.862691	20.325312
65.582991	2070.836771	20.330330
66.030572	2077.686962	20.335347
65.679761	2046.205973	20.340365
65.851893	2079.709406	20.345383
66.035153	2117.174515	20.350400
66.077724	2102.033178	20.355418
65.760925	2088.827419	20.360435
66.261056	2071.173306	20.365453
66.180414	2109.220830	20.370471
66.179652	2104.622097	20.375488
66.221206	2075.100666	20.380506
66.363624	2108.310020	20.385523
66.097679	2081.739942	20.390541
66.744835	2064.226778	20.395559
66.074489	2124.966388	20.400576
66.545393	2114.852725	20.405594
66.274207	2094.998148	20.410611
66.101621	2086.192886	20.415629
66.797150	2115.414397	20.420647
66.566265	2123.903411	20.425664
66.621629	2105.300042	20.430682
67.245169	2077.033139	20.435699
67.115929	2125.025572	20.440717
67.108312	2117.339972	20.445735
66.827985	2102.760591	20.450752
67.235234	2078.870658	20.455770
66.990891	2122.446153	20.460787
66.947400	2112.777117	20.465805
67.544730	2151.169681	20.470823
67.517361	2135.443264	20.475840
67.655112	2119.389288	20.480858
67.484545	2167.533961	20.485875
67.134219	2141.435785	20.490893
67.870131	2124.175819	20.495911
67.636913	2169.265342	20.500928
67.561783	2135.273600	20.505946
67.970748	2144.303980	20.510963
67.500360	2171.515510	20.515981
68.130182	2142.309134	20.520999
68.433738	2144.485103	20.526016
68.086268	2166.718669	20.531034
68.693671	2156.788498	20.536051
68.195360	2162.613690	20.541069
68.615822	2144.430267	20.546087
68.550547	2173.890416	20.551104
68.506619	2151.410223	20.556122
68.468697	2167.595476	20.561139
68.677006	2141.393269	20.566157
68.560621	2144.186785	20.571175
68.629060	2167.013934	20.576192
68.693970	2137.623937	20.581210
68.746903	2181.495134	20.586227
69.005937	2158.047149	20.591245
69.169586	2181.140719	20.596263
68.934778	2188.219338	20.601280
69.437599	2165.281471	20.606298
69.506771	2202.920730	20.611315
69.497893	2175.099783	20.616333
69.445764	2184.641822	20.621351
69.580543	2168.193422	20.626368
69.388170	2196.709584	20.631386
69.685034	2174.735028	20.636403
69.487013	2171.390804	20.641421
69.855735	2181.391926	20.646439
69.415679	2184.680675	20.651456
69.548381	2177.502797	20.656474
69.637835	2173.389897	20.661491
69.632130	2192.201811	20.666509
69.672687	2171.539974	20.671527
69.935213	2201.593657	20.676544
69.897733	2187.714815	20.681562
70.224908	2214.125171	20.686579
69.958124	2205.960160	20.691597
70.770543	2192.834577	20.696615
70.526067	2187.612412	20.701632
70.336128	2209.990029	20.706650
70.527990	2190.338343	20.711667
70.478694	2198.036282	20.716685
70.375221	2218.007456	20.721703
70.722464	2187.069248	20.726720
70.579248	2240.310535	20.731738
70.468421	2223.656622	20.736755
71.413957	2207.262152	20.741773
71.390335	2247.098198	20.746791
71.301183	2226.998111	20.751808
71.259308	2227.125956	20.756826
71.759806	2211.395507	20.761843
71.370638	2244.129923	20.766861
71.511250	2204.147886	20.771879
71.720202	2244.342468	20.776896
71.265580	2221.923726	20.781914
71.797345	2221.285238	20.786931
71.776432	2212.922919	20.791949
71.745822	2227.828151	20.796967
72.229307	2193.784944	20.801984
71.850065	2248.220905	20.807002
71.780330	2226.871045	20.812019
71.836738	2204.240270	20.817037
71.610843	2249.248646	20.822055
71.996394	2206.814417	20.827072
71.562626	2240.984303	20.832090
71.699683	2235.784653	20.837107
71.367390	2239.910418	20.842125
72.245958	2217.207505	20.847143
72.326094	2248.036014	20.852160
71.726460	2272.633412	20.857178
72.780508	2246.165582	20.862195
72.850207	2301.381979	20.867213
72.774394	2273.317462	20.872231
73.295603	2251.937826	20.877248
72.798981	2302.945274	20.882266
73.028489	2255.656034	20.887283
72.932283	2282.986648	20.892301
73.280527	2254.215080	20.897319
73.182736	2288.845902	20.902336
73.315307	2265.949617	20.907354
73.474006	2265.931428	20.912371
73.368982	2276.001870	20.917389
73.221283	2256.419189	20.922407
73.394954	2280.260112	20.927424
73.528396	2279.315463	20.932442
73.672851	2261.685592	20.937459
73.347105	2266.907554	20.942477
73.507331	2265.801325	20.947495
73.356535	2283.980515	20.952512
73.918468	2282.964390	20.957530
73.832624	2282.345733	20.962547
73.285045	2310.121988	20.967565
73.555193	2293.120152	20.972583
73.514763	2320.452953	20.977600
74.433752	2319.817209	20.982618
74.358744	2311.353343	20.987635
73.994451	2341.907627	20.992653
74.559487	2320.270779	20.997671
74.689932	2320.194171	21.002688
74.343464	2344.560972	21.007706
74.730321	2312.408825	21.012723
74.771002	2319.730666	21.017741
75.112925	2323.815796	21.022759
74.945799	2321.416764	21.027776
74.872233	2319.341815	21.032794
75.162699	2316.877679	21.037811
75.375402	2356.298793	21.042829
75.154657	2327.354321	21.047847
75.575527	2355.129603	21.052864
75.510966	2352.883318	21.057882
75.518150	2349.717912	21.062899
75.988943	2325.127638	21.067917
75.378144	2335.994537	21.072935
75.885111	2326.409047	21.077952
75.736636	2327.596072	21.082970
75.767082	2333.278807	21.087987
75.659456	2343.613992	21.093005
75.797446	2335.783142	21.098023
75.841170	2323.798608	21.103040
75.729525	2336.547567	21.108058
76.015583	2341.990547	21.113075
76.176858	2328.276514	21.118093
76.030649	2335.827164	21.123111
76.259996	2343.908629	21.128128
76.222518	2361.867702	21.133146
76.411381	2361.471877	21.138163
76.404300	2361.546981	21.143181
76.592562	2373.085622	21.148199
77.208615	2364.807268	21.153216
76.966017	2366.518205	21.158234
77.015873	2353.817692	21.163251
77.168523	2358.072234	21.168269
77.035523	2363.980043	21.173287
77.412239	2349.653518	21.178304
77.324473	2351.943835	21.183322
77.080233	2351.243463	21.188339
77.074755	2359.914544	21.193357
77.115244	2351.606064	21.198375
77.435049	2342.667854	21.203392
77.150984	2348.414120	21.208410
77.253174	2359.306558	21.213427
77.637415	2376.450388	21.218445
77.426613	2376.528876	21.223463
77.599008	2359.442659	21.228480
77.419560	2381.831451	21.233498
77.692521	2372.828330	21.238515
77.596947	2380.823983	21.243533
77.971572	2390.490024	21.248551
78.193015	2390.954212	21.253568
78.149405	2409.630873	21.258586
78.284933	2403.084038	21.263603
78.355450	2399.498726	21.268621
78.601223	2397.395653	21.273639
78.604459	2401.437281	21.278656
78.262425	2395.797992	21.283674
78.585692	2399.991518	21.288691
78.682022	2403.841327	21.293709
78.945351	2424.134984	21.298727
79.371146	2422.420075	21.303744
78.874009	2420.282088	21.308762
79.378321	2420.864774	21.313779
79.618277	2411.654521	21.318797
79.319657	2414.949081	21.323815
79.115991	2407.886867	21.328832
79.232452	2411.858530	21.333850
79.688654	2414.293360	21.338867
79.757794	2415.245905	21.343885
79.406040	2410.855637	21.348903
79.594967	2416.494256	21.353920
79.767551	2422.397405	21.358938
79.794211	2404.421970	21.363955
79.869912	2412.581461	21.368973
79.762671	2414.980292	21.373991
80.182649	2408.608330	21.379008
80.071545	2408.285507	21.384026
80.049816	2415.854889	21.389043
80.291200	2433.882060	21.394061
79.913074	2453.522953	21.399079
80.239137	2438.787543	21.404096
80.234704	2432.400661	21.409114
80.470771	2447.459446	21.414131
80.692971	2434.533954	21.419149
80.507106	2428.668389	21.424167
80.853083	2470.730270	21.429184
81.072780	2453.024458	21.434202
81.024032	2458.661666	21.439219
80.861204	2473.011686	21.444237
80.795175	2460.735423	21.449255
81.263405	2446.181054	21.454272
81.133385	2461.041813	21.459290
80.871011	2469.433009	21.464307
81.246346	2460.890163	21.469325
81.234370	2491.654435	21.474343
81.489450	2493.832683	21.479360
81.760892	2493.267161	21.484378
81.403690	2479.975458	21.489395
81.711902	2497.191334	21.494413
81.788166	2480.003107	21.499431
82.214370	2480.131822	21.504448
82.168525	2498.519499	21.509466
82.110751	2481.084429	21.514483
82.704158	2485.108266	21.519501
82.649705	2489.589366	21.524519
82.743009	2467.405357	21.529536
82.361055	2490.386638	21.534554
82.747865	2484.062407	21.539571
82.696456	2469.232208	21.544589
82.572951	2498.718031	21.549607
82.862696	2480.224681	21.554624
82.654168	2467.046143	21.559642
82.478659	2500.607557	21.564659
82.753659	2513.029158	21.569677
82.946802	2502.487586	21.574695
82.681031	2520.920587	21.579712
82.895382	2495.394011	21.584730
83.017238	2529.168424	21.589747
83.436237	2524.296543	21.594765
83.105963	2530.217786	21.599783
83.562820	2543.930263	21.604800
83.697146	2522.064480	21.609818
83.183053	2555.391344	21.614835
83.711676	2531.412887	21.619853
83.677205	2544.815153	21.624871
84.235486	2567.774046	21.629888
84.422921	2556.084177	21.634906
84.158720	2572.133705	21.639923
84.335892	2563.745103	21.644941
84.296672	2545.145243	21.649959
84.586262	2573.439773	21.654976
85.025034	2539.841794	21.659994
84.764105	2570.530307	21.665011
85.136542	2541.895896	21.670029
84.866540	2560.608065	21.675047
85.178934	2542.103946	21.680064
85.065891	2533.686130	21.685082
84.759894	2544.464462	21.690099
85.093777	2522.798104	21.695117
84.750623	2566.602269	21.700135
85.218711	2527.784725	21.705152
85.297398	2555.924865	21.710170
85.226304	2534.170476	21.715187
85.216222	2549.816066	21.720205
85.264495	2544.418092	21.725223
85.359444	2555.267785	21.730240
85.478302	2577.663582	21.735258
85.346136	2576.171346	21.740275
86.145392	2585.585750	21.745293
85.509446	2567.110120	21.750311
85.784133	2589.816163	21.755328
86.164757	2574.505590	21.760346
85.562847	2574.281479	21.765363
86.134666	2570.615400	21.770381
86.015525	2606.959587	21.775399
86.459511	2602.218198	21.780416
86.089421	2593.732791	21.785434
86.221387	2614.643092	21.790451
86.666152	2581.773995	21.795469
86.341566	2618.261090	21.800487
86.911634	2609.904984	21.805504
86.844786	2627.037667	21.810522
87.142193	2633.698127	21.815539
87.529335	2630.567246	21.820557
87.283416	2623.806626	21.825575
87.344810	2613.227778	21.830592
87.565925	2624.012570	21.835610
87.466624	2624.168452	21.840627
87.862005	2612.231433	21.845645
87.697157	2627.178930	21.850663
87.897890	2607.599205	21.855680
87.750993	2634.547639	21.860698
87.828494	2613.038443	21.865715
87.775538	2620.148050	21.870733
88.176245	2595.242074	21.875751
87.728583	2632.009969	21.880768
87.763758	2604.809641	21.885786
87.368664	2637.877815	21.890803
87.802286	2635.371921	21.895821
88.304754	2637.576028	21.900839
88.209043	2642.092071	21.905856
88.559757	2668.436576	21.910874
88.608971	2657.938295	21.915891
88.978330	2649.907563	21.920909
89.191930	2670.858414	21.925927
89.757638	2643.401944	21.930944
89.860979	2635.416785	21.935962
89.272474	2634.455880	21.940979
89.654030	2622.647694	21.945997
89.302517	2608.051623	21.951015
89.262276	2633.869271	21.956032
89.739048	2591.717485	21.961050
89.405169	2637.375105	21.966067
89.493156	2603.655152	21.971085
89.637023	2659.213463	21.976103
89.933701	2640.039210	21.981120
89.817947	2660.222175	21.986138
90.034830	2654.149928	21.991155
90.075755	2662.337916	21.996173
89.957714	2646.786651	22.001191
89.897258	2662.808509	22.006208
90.321957	2637.083749	22.011226
90.138131	2652.609281	22.016243
90.027928	2679.080790	22.021261
90.335222	2691.595716	22.026279
90.207722	2681.802047	22.031296
90.354259	2705.142231	22.036314
90.257909	2688.575932	22.041331
90.486587	2716.082870	22.046349
91.032407	2693.042934	22.051367
90.967994	2732.209575	22.056384
91.352361	2690.425412	22.061402
91.200483	2728.591314	22.066419
91.665696	2694.162864	22.071437
91.439766	2728.154444	22.076455
91.704061	2693.124843	22.081472
91.758906	2714.521889	22.086490
91.713657	2684.227279	22.091507
92.010735	2701.202123	22.096525
91.884621	2696.655440	22.101543
92.036951	2700.196715	22.106560
92.063292	2677.806756	22.111578
92.332058	2708.278950	22.116595
92.349343	2711.860640	22.121613
92.095321	2714.912969	22.126631
92.295256	2697.777130	22.131648
92.427260	2735.791597	22.136666
92.050978	2707.262095	22.141683
92.448009	2719.793412	22.146701
92.285170	2731.689583	22.151719
92.905258	2737.010231	22.156736
92.787807	2726.686352	22.161754
92.801694	2762.365511	22.166771
92.920453	2722.448463	22.171789
92.983524	2750.982396	22.176807
93.111265	2740.331524	22.181824
93.360422	2744.168853	22.186842
93.443035	2763.919178	22.191859
93.216857	2778.680753	22.196877
93.629759	2762.272284	22.201895
93.274763	2786.011133	22.206912
93.834199	2775.434555	22.211930
93.893519	2766.776743	22.216947
94.124818	2812.373103	22.221965
94.344599	2784.771738	22.226983
94.170599	2818.476013	22.232000
94.579127	2770.722366	22.237018
94.465978	2810.229709	22.242035
94.323700	2781.167991	22.247053
94.901070	2796.100350	22.252071
94.599437	2784.307372	22.257088
94.711178	2801.576963	22.262106
94.922345	2787.027852	22.267123
94.542982	2795.005271	22.272141
94.860937	2807.309368	22.277159
94.845161	2805.858329	22.282176
95.348077	2808.649966	22.287194
95.259046	2828.763617	22.292211
95.474831	2796.193268	22.297229
95.545866	2827.364258	22.302247
95.597367	2806.053995	22.307264
95.576509	2814.751397	22.312282
95.635212	2803.354800	22.317299
95.729003	2801.271973	22.322317
95.723014	2829.091061	22.327335
95.697499	2824.020168	22.332352
96.167492	2857.100341	22.337370
95.890986	2846.432048	22.342387
96.241073	2845.583391	22.347405
96.313531	2837.846886	22.352423
96.174937	2849.752659	22.357440
96.263989	2846.273617	22.362458
96.439653	2852.444675	22.367475
96.253175	2886.674959	22.372493
96.559140	2854.675317	22.377511
96.352882	2888.249605	22.382528
96.987057	2867.354472	22.387546
97.087858	2915.903550	22.392563
97.091787	2879.695816	22.397581
97.775869	2902.018502	22.402599
98.026295	2883.121890	22.407616
97.848196	2903.427614	22.412634
97.989039	2866.807936	22.417651
98.026806	2903.059408	22.422669
98.147278	2871.577774	22.427687
97.743576	2898.042994	22.432704
98.273655	2876.847455	22.437722
98.154464	2875.277607	22.442739
98.051814	2891.521967	22.447757
98.133866	2876.600851	22.452775
98.014808	2887.079828	22.457792
98.456486	2867.520329	22.462810
98.155384	2883.086042	22.467827
98.099850	2921.047519	22.472845
98.737740	2890.861432	22.477863
98.726002	2891.865447	22.482880
99.088734	2920.871073	22.487898
98.913795	2897.185908	22.492915
99.021040	2891.871219	22.497933
99.329091	2933.899587	22.502951
99.299525	2926.389321	22.507968
99.511438	2931.547020	22.512986
99.803439	2931.741979	22.518003
99.663667	2911.125153	22.523021
99.758362	2949.328613	22.528039
99.686702	2924.741240	22.533056
99.809213	2942.850926	22.538074
99.723902	2916.897086	22.543091
99.617378	2950.034792	22.548109
100.384084	2924.371408	22.553127
100.686805	2968.355385	22.558144
100.584193	2937.986016	22.563162
101.027323	2972.593564	22.568179
100.801061	2939.685144	22.573197
100.935633	2932.172301	22.578215
100.968171	2972.673905	22.583232
100.774650	2935.485182	22.588250
101.100683	2925.773987	22.593267
100.777431	2968.765216	22.598285
100.954470	2933.660068	22.603303
100.917996	2952.542371	22.608320
101.260183	2936.730990	22.613338
101.244585	2942.358378	22.618355
101.255754	2945.407797	22.623373
101.262094	2990.076232	22.628391
100.636942	2979.633337	22.633408
101.744205	2974.570544	22.638426
101.350928	2980.323457	22.643443
101.539880	2981.072873	22.648461
102.122342	3009.166595	22.653479
101.932612	3010.335080	22.658496
102.238021	2976.747926	22.663514
102.522865	3019.647846	22.668531
102.790416	2999.317550	22.673549
102.987518	3035.500683	22.678567
102.955605	3042.571743	22.683584
103.063964	3011.072075	22.688602
103.561685	2996.057027	22.693619
103.093360	3022.403775	22.698637
102.988852	2992.453847	22.703655
103.350329	3011.128826	22.708672
103.074435	3022.786046	22.713690
103.326545	2992.776892	22.718707
103.515406	3020.621124	22.723725
103.558640	3019.190544	22.728743
103.610650	3038.766779	22.733760
103.775347	3003.989078	22.738778
103.857134	3029.903597	22.743795
104.143452	3042.398573	22.748813
104.154262	3034.966765	22.753831
103.954366	3073.586435	22.758848
104.640205	3039.398874	22.763866
104.082083	3067.033509	22.768883
104.439899	3027.554183	22.773901
104.561168	3054.903481	22.778919
104.172817	3049.504936	22.783936
104.438367	3088.567217	22.788954
105.142313	3074.728984	22.793971
104.734732	3097.237841	22.798989
105.271127	3071.415851	22.804007
105.147545	3071.588194	22.809024
105.355774	3092.143282	22.814042
105.798890	3083.918064	22.819059
105.752632	3109.046884	22.824077
106.165833	3070.191819	22.829095
106.059488	3111.627614	22.834112
105.970439	3087.655495	22.839130
105.979982	3079.691344	22.844147
106.080158	3082.646366	22.849165
106.260785	3102.145543	22.854183
106.098759	3077.256898	22.859200
106.151517	3104.277406	22.864218
106.380152	3095.142471	22.869235
105.879423	3097.062979	22.874253
106.688491	3097.929049	22.879271
106.259134	3104.420867	22.884288
106.398660	3138.413336	22.889306
106.736474	3120.673723	22.894323
106.480611	3122.799034	22.899341
107.036131	3123.140760	22.904359
106.975323	3151.936715	22.909376
107.325632	3138.545749	22.914394
107.410610	3152.277202	22.919411
107.434579	3151.860456	22.924429
107.917485	3132.364824	22.929447
107.630103	3138.135523	22.934464
107.724836	3168.942417	22.939482
108.066010	3165.718072	22.944499
107.898141	3164.380920	22.949517
107.978664	3178.737665	22.954535
108.049272	3184.839878	22.959552
108.084917	3164.282035	22.964570
108.438079	3200.478449	22.969587
108.583184	3199.069365	22.974605
108.747236	3193.457614	22.979623
108.956688	3181.539555	22.984640
108.598905	3216.792186	22.989658
108.868326	3196.097123	22.994675
108.690266	3197.946529	22.999693
108.833977	3232.954835	23.004711
109.343536	3219.639873	23.009728
109.231062	3218.902711	23.014746
109.554867	3228.526291	23.019763
109.377051	3221.427306	23.024781
109.660234	3249.718668	23.029799
110.087623	3249.416939	23.034816
110.215476	3233.721220	23.039834
110.251980	3249.842319	23.044851
110.520157	3226.136305	23.049869
110.695284	3230.701374	23.054887
110.585801	3238.907376	23.059904
111.034522	3238.145231	23.064922
111.124980	3219.073897	23.069939
111.021212	3241.899514	23.074957
110.910940	3234.148673	23.079975
110.995613	3225.069650	23.084992
110.998581	3227.068752	23.090010
111.256442	3225.120957	23.095027
111.250466	3230.871205	23.100045
111.359960	3242.992598	23.105063
111.196939	3269.832289	23.110080
111.625404	3265.458151	23.115098
111.852326	3256.482282	23.120115
111.433206	3285.418227	23.125133
112.110909	3253.815455	23.130151
111.628193	3260.264720	23.135168
111.990832	3283.342471	23.140186
112.155238	3289.451010	23.145203
112.028558	3284.506212	23.150221
112.266377	3304.352872	23.155239
112.361556	3286.707596	23.160256
112.342864	3288.444288	23.165274
112.577785	3311.459070	23.170291
112.571946	3324.350913	23.175309
112.720334	3304.498572	23.180327
112.718891	3316.856390	23.185344
113.173030	3338.525777	23.190362
113.298285	3320.643617	23.195379
113.346273	3348.772090	23.200397
113.271801	3335.782197	23.205415
113.538699	3331.177369	23.210432
113.785106	3336.790663	23.215450
113.738177	3367.834522	23.220467
114.007207	3357.550043	23.225485
114.131492	3358.291700	23.230503
114.219472	3380.960316	23.235520
114.341042	3355.185094	23.240538
114.555935	3355.866680	23.245555
114.292910	3379.845899	23.250573
114.546410	3362.462400	23.255591
114.794162	3373.392171	23.260608
114.740696	3386.160299	23.265626
114.794055	3390.223314	23.270643
114.687382	3397.842147	23.275661
115.453762	3382.607668	23.280679
115.664494	3371.217065	23.285696
115.017206	3406.458891	23.290714
115.459010	3397.821526	23.295731
115.569051	3416.471042	23.300749
115.726444	3409.934431	23.305767
115.950517	3407.736353	23.310784
115.798204	3408.541781	23.315802
116.364021	3419.073190	23.320819
116.213927	3443.471861	23.325837
116.437337	3428.801384	23.330855
116.599793	3441.550078	23.335872
116.368066	3447.507888	23.340890
116.763903	3436.235603	23.345907
116.550926	3454.215351	23.350925
116.885424	3437.863468	23.355943
117.029762	3470.712211	23.360960
117.246161	3454.415325	23.365978
117.523023	3487.410523	23.370995
117.361788	3472.325432	23.376013
117.508655	3460.911906	23.381031
117.711317	3470.329991	23.386048
117.702659	3447.061855	23.391066
117.890086	3470.986704	23.396083
118.295631	3443.787114	23.401101
118.163557	3445.781034	23.406119
118.312456	3466.820437	23.411136
118.360257	3456.027615	23.416154
118.471322	3443.724646	23.421171
118.500154	3489.852547	23.426189
118.507945	3462.490586	23.431207
118.679767	3483.107094	23.436224
118.525406	3479.658848	23.441242
118.604174	3464.830477	23.446259
118.542026	3504.227730	23.451277
118.669519	3493.989323	23.456295
118.991495	3514.996479	23.461312
119.194225	3499.810062	23.466330
119.209672	3523.336075	23.471347
119.398838	3516.449813	23.476365
119.695082	3545.816544	23.481383
119.733407	3548.156950	23.486400
119.969904	3523.468303	23.491418
119.893256	3550.528362	23.496435
120.050502	3545.447742	23.501453
120.745996	3538.415448	23.506471
120.409652	3586.472453	23.511488
120.321519	3568.445453	23.516506
121.216542	3538.461676	23.521523
120.843180	3578.889664	23.526541
121.132255	3534.580657	23.531559
121.164238	3560.007703	23.536576
121.021581	3531.471583	23.541594
121.404036	3577.253114	23.546611
121.480973	3560.300282	23.551629
121.544085	3597.376959	23.556647
121.668172	3557.994828	23.561664
121.530396	3599.253733	23.566682
121.916269	3570.018916	23.571699
122.093310	3581.509964	23.576717
121.880727	3587.853368	23.581735
122.381153	3595.804211	23.586752
122.008943	3585.471573	23.591770
122.245300	3611.238191	23.596787
122.341193	3614.576303	23.601805
122.548695	3605.645009	23.606823
122.674549	3613.824709	23.611840
122.926863	3637.471248	23.616858
123.131379	3619.588671	23.621875
123.277003	3630.897552	23.626893
123.295373	3613.235812	23.631911
123.598479	3649.373674	23.636928
123.445576	3646.159570	23.641946
124.017735	3642.232025	23.646963
124.142019	3663.819979	23.651981
124.633567	3646.025329	23.656999
124.496134	3662.254852	23.662016
124.338941	3637.356614	23.667034
124.596223	3668.185055	23.672051
124.596591	3650.843149	23.677069
124.391597	3635.879713	23.682087
125.060903	3608.522129	23.687104
124.972416	3654.741626	23.692122
124.332831	3637.809343	23.697139
124.327659	3642.339575	23.702157
125.076780	3616.581038	23.707175
125.250060	3666.859489	23.712192
124.982252	3650.267518	23.717210
125.077763	3671.341687	23.722227
125.320180	3658.528314	23.727245
125.057266	3704.364375	23.732263
125.780743	3674.579160	23.737280
125.304689	3707.617029	23.742298
125.913531	3686.106491	23.747315
125.857816	3739.034867	23.752333
126.025346	3725.735442	23.757351
126.550577	3720.633060	23.762368
126.240939	3762.514517	23.767386
126.416469	3749.346735	23.772403
126.504853	3757.940750	23.777421
127.231948	3739.840977	23.782439
127.260785	3754.108987	23.787456
127.160208	3780.659618	23.792474
127.024105	3758.110621	23.797491
127.501437	3747.168862	23.802509
127.427175	3775.508799	23.807527
127.697442	3790.349560	23.812544
127.767201	3765.897122	23.817562
128.000295	3796.625069	23.822579
128.017049	3775.286682	23.827597
128.010149	3781.209565	23.832615
128.292424	3832.998842	23.837632
128.320961	3834.244289	23.842650
128.311218	3799.136956	23.847667
128.655464	3812.172428	23.852685
128.499999	3815.280062	23.857703
129.387970	3794.841089	23.862720
129.253329	3850.944707	23.867738
129.372375	3804.506621	23.872755
129.565388	3844.503637	23.877773
129.465120	3837.499754	23.882791
129.666219	3795.399478	23.887808
129.698453	3838.832942	23.892826
129.869022	3814.807222	23.897843
130.059778	3850.873034	23.902861
130.112265	3839.113198	23.907879
130.194907	3853.958767	23.912896
130.486033	3843.330602	23.917914
130.277226	3872.116173	23.922931
130.920678	3849.666143	23.927949
130.368993	3856.351637	23.932967
130.456502	3876.078301	23.937984
130.665541	3856.259594	23.943002
130.770865	3891.881308	23.948019
130.950994	3866.852592	23.953037
131.254531	3918.298168	23.958055
131.603091	3896.624298	23.963072
131.367989	3908.880637	23.968090
131.804623	3895.907083	23.973107
131.950621	3910.340638	23.978125
131.895090	3882.114036	23.983143
131.872627	3928.773038	23.988160
131.796241	3916.216372	23.993178
132.211479	3905.027954	23.998195
132.101888	3928.075826	24.003213
132.358935	3932.327560	24.008231
132.581131	3925.664753	24.013248
132.620460	3965.701550	24.018266
132.538105	3932.778172	24.023283
133.017442	3973.971203	24.028301
133.388239	3956.598979	24.033319
133.350700	3968.507639	24.038336
133.716922	3985.029294	24.043354
134.042486	3956.544340	24.048371
134.060662	3984.519101	24.053389
133.796449	3961.225602	24.058407
134.022183	3990.869569	24.063424
134.175979	3956.730097	24.068442
134.118148	3974.875325	24.073459
134.569329	4001.143295	24.078477
134.076657	4007.846979	24.083495
134.688602	3981.695906	24.088512
134.404419	4015.617163	24.093530
134.767030	4005.752325	24.098547
134.827415	4035.945863	24.103565
134.895316	4022.890181	24.108583
135.183191	4039.260768	24.113600
135.636697	4042.405870	24.118618
135.450688	4067.272278	24.123635
136.204773	4041.441413	24.128653
135.970328	4050.238894	24.133671
136.655445	4025.972674	24.138688
136.496306	4070.170487	24.143706
136.005471	4045.895068	24.148723
136.159195	4042.502190	24.153741
136.553419	4057.047348	24.158759
136.550251	4058.541729	24.163776
136.866930	4055.784434	24.168794
137.384511	4041.507751	24.173811
137.485343	4068.014989	24.178829
137.448701	4096.943466	24.183847
137.326514	4066.770747	24.188864
137.553306	4055.607541	24.193882
137.799891	4108.814724	24.198899
138.071446	4078.847448	24.203917
137.913911	4124.289642	24.208935
138.489574	4085.738739	24.213952
138.397034	4105.002765	24.218970
137.774972	4112.885071	24.223987
138.230655	4084.560837	24.229005
138.060636	4119.506438	24.234023
138.564240	4120.288348	24.239040
138.746989	4142.773906	24.244058
138.827271	4130.568881	24.249075
138.953622	4129.441960	24.254093
139.119367	4122.546564	24.259111
139.331634	4175.060916	24.264128
139.544552	4154.287769	24.269146
139.600449	4160.649184	24.274163
139.888143	4149.126139	24.279181
139.889565	4160.821067	24.284199
139.759267	4167.443447	24.289216
140.148349	4155.482587	24.294234
140.219694	4193.583678	24.299251
140.407747	4187.204671	24.304269
140.597767	4171.716727	24.309287
140.810126	4167.725270	24.314304
140.702604	4192.531391	24.319322
140.966579	4212.047082	24.324339
141.339242	4204.136128	24.329357
141.238711	4208.545648	24.334375
140.951579	4212.601034	24.339392
141.459557	4219.026485	24.344410
141.431110	4236.764585	24.349427
142.073383	4225.987333	24.354445
141.708095	4224.685490	24.359463
142.172925	4215.610534	24.364480
142.382489	4257.523899	24.369498
142.446474	4227.122930	24.374515
142.844799	4259.992736	24.379533
142.676364	4272.923138	24.384551
142.777385	4255.034263	24.389568
142.908564	4258.853837	24.394586
142.797444	4273.176133	24.399603
143.104923	4251.294321	24.404621
142.856944	4285.481825	24.409639
143.199357	4280.520108	24.414656
143.220223	4283.588713	24.419674
143.413638	4309.532541	24.424691
143.921363	4294.297464	24.429709
144.042427	4292.610488	24.434727
144.216630	4323.155413	24.439744
144.828775	4318.830351	24.444762
144.845940	4312.801853	24.449779
145.422144	4320.045609	24.454797
145.368970	4328.677476	24.459815
145.317618	4329.647787	24.464832
145.509689	4315.966319	24.469850
145.373965	4309.966918	24.474867
145.597529	4314.744085	24.479885
145.676954	4324.677968	24.484903
145.444708	4312.960789	24.489920
145.246212	4311.383760	24.494938
145.337590	4346.099426	24.499955
146.036653	4343.668935	24.504973
145.703154	4339.530039	24.509991
146.070923	4361.114814	24.515008
146.532174	4357.484821	24.520026
146.661486	4355.560526	24.525043
146.971402	4372.890845	24.530061
146.982244	4359.285432	24.535079
147.280818	4375.418693	24.540096
147.286100	4384.943573	24.545114
146.720529	4369.671077	24.550131
147.574440	4375.288610	24.555149
147.433401	4387.143311	24.560167
147.725496	4399.614935	24.565184
147.647041	4396.303047	24.570202
147.824942	4393.066714	24.575219
147.508095	4423.740486	24.580237
148.205171	4399.828892	24.585255
148.302536	4442.633870	24.590272
148.528451	4458.564835	24.595290
148.315755	4461.337168	24.600307
149.273379	4437.285640	24.605325
149.032229	4468.463488	24.610343
149.434565	4443.816869	24.615360
149.422990	4447.018907	24.620378
149.645905	4496.909974	24.625395
149.330697	4455.239405	24.630413
149.725062	4492.917680	24.635431
149.797450	4463.269296	24.640448
150.068544	4489.186898	24.645466
150.374265	4492.052010	24.650483
150.327956	4513.566149	24.655501
150.596742	4502.537511	24.660519
150.570684	4504.397455	24.665536
150.741975	4518.535724	24.670554
150.834037	4504.423985	24.675571
151.048156	4545.587753	24.680589
151.358830	4533.598969	24.685607
151.264976	4507.045801	24.690624
151.315526	4547.253103	24.695642
151.714723	4540.853654	24.700659
151.747823	4575.636581	24.705677
151.654030	4553.893031	24.710695
151.663023	4592.111298	24.715712
152.422718	4560.370722	24.720730
152.317500	4590.251963	24.725747
153.078509	4582.263945	24.730765
152.438762	4581.293748	24.735783
153.230145	4576.309126	24.740800
153.349816	4582.872958	24.745818
153.428756	4629.090856	24.750835
153.386997	4614.294701	24.755853
154.000047	4593.958251	24.760871
153.670052	4627.374525	24.765888
154.175448	4580.185621	24.770906
154.033760	4621.201794	24.775923
154.577685	4598.978113	24.780941
154.465420	4637.082883	24.785959
154.632757	4622.902389	24.790976
154.522514	4621.176734	24.795994
154.500319	4630.664461	24.801011
154.379705	4633.621174	24.806029
154.732060	4636.928858	24.811047
154.935487	4644.054424	24.816064
154.752920	4666.119157	24.821082
155.070315	4653.764186	24.826099
155.071683	4674.122412	24.831117
155.296106	4684.979794	24.836135
155.573273	4677.201816	24.841152
156.158406	4686.922368	24.846170
155.917209	4720.603967	24.851187
156.518144	4694.129278	24.856205
156.244298	4723.350903	24.861223
156.848136	4687.577996	24.866240
157.013382	4739.076037	24.871258
157.070306	4721.833197	24.876275
157.113452	4746.299985	24.881293
157.116161	4714.377682	24.886311
157.298795	4740.756667	24.891328
157.530147	4726.414038	24.896346
157.418481	4784.443351	24.901363
157.810730	4757.959338	24.906381
158.008129	4757.067275	24.911399
157.817379	4771.912522	24.916416
158.176993	4793.651853	24.921434
158.500684	4782.802270	24.926451
158.828697	4778.885827	24.931469
158.887621	4790.479261	24.936487
159.130517	4822.382316	24.941504
159.302623	4796.082803	24.946522
159.245014	4833.488658	24.951539
159.643665	4814.470746	24.956557
159.461134	4818.085595	24.961575
159.575297	4825.651078	24.966592
159.993169	4849.825436	24.971610
160.081093	4839.542053	24.976627
160.175551	4826.712709	24.981645
160.611546	4868.779739	24.986663
160.312926	4890.178104	24.991680
160.338717	4877.208620	24.996698
160.873420	4850.613620	25.001715
160.951061	4896.356620	25.006733
161.045027	4874.468591	25.011751
161.634004	4861.245700	25.016768
161.977495	4901.301065	25.021786
161.747048	4894.167173	25.026803
162.284038	4870.241795	25.031821
162.056339	4909.195629	25.036839
162.157286	4924.531046	25.041856
162.543321	4898.903690	25.046874
162.554791	4941.952745	25.051891
162.261584	4911.018077	25.056909
162.878214	4928.219127	25.061927
162.442002	4928.881876	25.066944
163.207090	4949.121869	25.071962
163.424538	4936.249221	25.076979
163.559121	4975.390131	25.081997
163.489682	4948.598624	25.087015
163.788819	4922.266046	25.092032
163.865195	4978.511038	25.097050
163.768259	4962.739175	25.102067
164.143666	4985.089107	25.107085
164.461112	4964.111708	25.112103
164.404865	4997.000573	25.117120
164.632359	4973.811942	25.122138
164.370048	5016.174811	25.127155
164.956380	5008.207338	25.132173
165.024056	5008.996657	25.137191
165.061532	5011.418462	25.142208
165.222953	5044.217661	25.147226
165.444545	5031.200304	25.152243
165.389711	5055.818539	25.157261
165.906179	5033.593864	25.162279
165.793327	5083.608897	25.167296
166.065601	5053.860587	25.172314
166.331889	5100.596853	25.177331
166.398635	5089.314417	25.182349
167.163650	5063.124443	25.187367
167.166770	5116.376455	25.192384
167.193820	5084.341691	25.197402
167.496934	5077.736270	25.202419
167.283812	5132.587559	25.207437
167.956296	5099.517621	25.212455
167.715527	5136.198214	25.217472
167.613836	5094.530337	25.222490
167.931349	5156.813249	25.227507
167.923346	5148.473155	25.232525
168.708033	5120.682150	25.237543
168.289436	5158.363512	25.242560
168.841241	5137.771749	25.247578
169.201720	5181.538404	25.252595
169.279325	5147.675009	25.257613
169.583506	5170.104235	25.262631
169.313391	5160.538541	25.267648
170.127968	5143.857275	25.272666
170.142787	5168.352882	25.277683
169.867305	5196.334286	25.282701
170.382184	5160.609820	25.287719
170.152192	5169.922547	25.292736
170.302328	5178.156681	25.297754
170.524104	5194.289715	25.302771
170.595108	5234.168365	25.307789
170.944875	5203.467284	25.312807
171.193806	5199.297434	25.317824
171.505585	5204.092299	25.322842
171.458000	5249.594388	25.327859
171.424076	5218.013545	25.332877
172.052941	5244.935925	25.337895
171.532584	5249.242757	25.342912
171.998421	5222.868119	25.347930
172.386591	5279.851262	25.352947
171.809419	5272.178496	25.357965
173.000035	5243.487847	25.362983
172.724968	5306.379586	25.368000
172.790487	5279.798826	25.373018
173.454909	5261.438142	25.378035
173.273713	5307.129279	25.383053
173.500082	5299.152170	25.388071
173.891446	5278.983079	25.393088
173.791793	5306.539372	25.398106
173.859338	5329.598174	25.403123
173.878146	5310.052509	25.408141
174.235083	5284.434632	25.413159
174.064756	5345.525581	25.418176
174.602342	5333.031882	25.423194
174.699958	5325.238922	25.428211
174.728615	5348.382624	25.433229
174.885804	5385.162454	25.438247
174.886566	5365.991708	25.443264
175.206446	5373.236739	25.448282
175.308049	5421.917504	25.453299
175.251450	5425.916797	25.458317
175.767596	5437.334001	25.463335
175.843792	5454.641499	25.468352
176.226836	5449.540750	25.473370
176.563299	5432.890542	25.478387
176.661887	5461.625491	25.483405
177.201703	5453.123937	25.488423
177.556974	5465.593479	25.493440
177.156960	5456.690265	25.498458
177.873994	5451.809261	25.503475
177.731484	5473.200103	25.508493
178.395630	5487.167113	25.513511
178.406302	5471.367322	25.518528
178.444219	5501.320423	25.523546
178.396644	5478.160693	25.528563
178.630778	5465.786852	25.533581
178.802683	5496.214215	25.538599
178.369312	5481.457592	25.543616
178.840228	5501.359759	25.548634
179.150038	5510.392321	25.553651
179.367268	5500.341976	25.558669
179.266884	5536.355284	25.563687
179.684962	5529.672330	25.568704
179.575338	5525.749938	25.573722
180.206958	5553.463102	25.578739
180.012995	5570.678489	25.583757
180.491341	5559.719505	25.588775
180.265586	5556.456799	25.593792
180.423831	5583.067759	25.598810
180.777606	5583.108166	25.603827
180.941710	5591.037416	25.608845
181.080137	5598.644272	25.613863
181.247205	5637.631499	25.618880
181.252546	5631.136243	25.623898
181.455881	5624.980760	25.628915
181.754716	5651.878616	25.633933
182.134878	5620.523559	25.638951
182.106801	5654.853832	25.643968
182.358736	5648.616640	25.648986
182.830499	5683.194572	25.654003
183.144552	5669.877118	25.659021
183.367565	5671.913065	25.664039
183.262854	5681.380793	25.669056
183.361337	5682.090498	25.674074
183.753954	5669.873743	25.679092
183.547443	5718.351279	25.684109
184.005268	5693.147742	25.689127
184.228883	5701.629291	25.694144
184.391898	5696.503745	25.699162
184.753217	5732.938781	25.704180
184.652252	5710.986180	25.709197
184.853442	5732.607401	25.714215
185.260618	5722.855479	25.719232
185.189176	5722.367331	25.724250
185.523058	5758.697450	25.729268
185.803288	5736.568389	25.734285
186.131792	5736.916506	25.739303
185.893904	5756.926511	25.744320
186.313264	5747.107331	25.749338
186.312462	5770.759116	25.754356
186.736118	5754.432156	25.759373
186.811440	5781.656974	25.764391
187.002569	5743.748384	25.769408
187.426053	5750.977874	25.774426
187.315153	5763.689563	25.779444
187.057305	5780.837492	25.784461
187.393066	5821.683333	25.789479
187.166009	5822.828084	25.794496
187.729232	5812.025319	25.799514
188.116873	5849.048860	25.804532
187.997698	5863.264627	25.809549
188.148927	5844.130638	25.814567
188.239877	5896.714538	25.819584
188.366912	5882.365392	25.824602
189.024348	5898.000972	25.829620
188.991457	5920.010672	25.834637
189.851369	5888.765812	25.839655
189.850524	5913.708876	25.844672
189.479891	5931.334417	25.849690
190.366397	5928.452900	25.854708
190.315541	5937.226165	25.859725
190.470629	5952.704291	25.864743
190.426721	5960.757377	25.869760
190.958466	5944.955833	25.874778
190.848943	5948.221802	25.879796
191.030645	5987.125798	25.884813
191.286131	5966.952259	25.889831
191.532693	6000.757278	25.894848
191.589329	5982.741998	25.899866
191.922926	5986.429838	25.904884
191.844779	5975.254007	25.909901
192.211894	6018.878906	25.914919
192.569172	6002.625983	25.919936
192.583097	6037.066100	25.924954
193.009003	6007.553369	25.929972
192.713094	6045.575399	25.934989
193.274050	6037.020581	25.940007
193.092996	6061.618916	25.945024
193.574745	6051.705409	25.950042
193.657601	6074.878587	25.955060
193.913469	6074.974731	25.960077
193.904113	6096.876305	25.965095
194.278635	6076.571135	25.970112
194.246537	6099.829552	25.975130
194.541376	6100.953277	25.980148
194.890007	6110.072072	25.985165
195.015893	6141.607197	25.990183
195.185451	6114.330168	25.995200
194.964255	6151.933809	26.000218
195.661501	6144.082592	26.005236
195.625658	6158.303452	26.010253
195.794252	6179.075320	26.015271
195.937308	6193.178790	26.020288
196.214081	6161.607765	26.025306
196.475965	6212.670702	26.030324
196.671563	6248.924941	26.035341
196.625231	6232.449728	26.040359
197.293776	6215.381435	26.045376
197.459200	6216.439257	26.050394
197.871680	6256.333107	26.055412
198.084357	6245.870721	26.060429
198.598438	6251.976684	26.065447
198.725321	6289.363898	26.070464
198.648080	6279.261625	26.075482
199.053728	6251.048224	26.080500
199.262153	6269.099544	26.085517
199.009861	6253.274749	26.090535
199.688620	6277.146305	26.095552
199.553644	6267.472587	26.100570
199.548521	6307.481140	26.105588
199.895031	6275.697344	26.110605
199.861890	6316.473547	26.115623
200.784765	6297.828851	26.120640
200.018662	6334.692933	26.125658
200.494709	6319.972233	26.130676
200.684175	6339.780360	26.135693
200.742959	6345.489245	26.140711
200.985740	6343.366437	26.145728
200.936105	6369.900235	26.150746
201.437414	6383.113589	26.155764
201.478950	6411.278060	26.160781
201.675250	6406.021082	26.165799
202.319117	6392.054033	26.170816
202.374507	6398.001083	26.175834
202.850037	6411.049418	26.180852
202.979549	6404.002171	26.185869
202.889587	6431.559014	26.190887
203.443932	6387.723139	26.195904
203.297920	6447.483552	26.200922
203.185823	6420.303573	26.205940
203.698392	6433.635555	26.210957
203.661074	6470.930602	26.215975
203.771689	6444.699328	26.220992
203.938857	6468.875406	26.226010
204.279396	6491.518786	26.231028
204.782017	6492.956388	26.236045
204.831111	6507.219117	26.241063
205.024520	6510.029369	26.246080
205.060324	6519.907172	26.251098
205.372348	6528.134352	26.256116
205.849582	6537.391841	26.261133
205.777640	6545.001251	26.266151
205.706128	6547.054376	26.271168
206.213879	6577.509894	26.276186
206.429189	6567.982342	26.281204
206.647859	6590.148058	26.286221
206.650470	6612.309697	26.291239
207.049367	6605.396437	26.296256
206.683509	6620.617633	26.301274
207.301862	6637.989580	26.306292
207.876185	6653.414984	26.311309
208.079126	6647.919254	26.316327
208.027091	6678.087348	26.321344
208.492178	6673.885778	26.326362
208.606564	6690.990368	26.331380
209.106105	6682.407208	26.336397
208.879686	6689.881600	26.341415
209.797110	6716.377516	26.346432
209.512694	6723.444961	26.351450
209.672213	6719.986035	26.356468
209.653914	6724.786815	26.361485
209.817470	6733.603476	26.366503
210.466258	6742.893544	26.371520
210.541521	6745.710873	26.376538
210.577441	6778.712534	26.381556
210.847854	6777.666310	26.386573
210.909868	6777.261495	26.391591
211.348529	6782.462310	26.396608
211.493702	6806.873762	26.401626
211.740989	6822.477364	26.406644
212.040410	6814.268285	26.411661
212.138782	6833.570739	26.416679
212.333678	6856.215866	26.421696
212.313537	6853.996424	26.426714
212.461388	6854.734510	26.431732
212.869969	6869.960754	26.436749
212.685344	6879.087140	26.441767
213.219816	6885.040630	26.446784
213.374412	6898.856541	26.451802
213.119872	6902.334667	26.456820
213.593976	6932.318695	26.461837
213.868546	6938.471783	26.466855
214.171930	6938.978152	26.471872
214.370118	6970.128215	26.476890
214.527464	6965.066082	26.481908
215.122918	6964.466076	26.486925
215.026244	6985.016998	26.491943
215.712952	6979.808318	26.496960
215.463117	6993.318205	26.501978
215.567048	7007.881100	26.506996
215.477098	7030.505021	26.512013
215.851352	7037.674546	26.517031
216.175434	7052.196096	26.522048
216.620275	7071.357082	26.527066
216.774152	7077.686828	26.532084
217.165546	7090.771996	26.537101
217.050378	7108.687877	26.542119
217.565805	7101.834495	26.547136
218.068248	7122.013934	26.552154
218.356123	7130.093446	26.557172
218.522663	7129.502010	26.562189
218.594363	7131.593757	26.567207
218.858622	7142.350615	26.572224
218.884641	7157.251029	26.577242
219.046140	7161.845469	26.582260
219.296208	7163.449291	26.587277
219.078249	7181.378497	26.592295
219.683132	7189.822159	26.597312
220.006437	7195.726035	26.602330
219.817679	7214.778915	26.607348
220.509421	7221.602865	26.612365
220.473844	7241.543277	26.617383
220.999832	7242.007880	26.622400
221.215737	7256.139306	26.627418
221.365853	7264.497354	26.632436
221.872435	7273.524027	26.637453
221.703929	7280.281349	26.642471
221.935959	7278.566909	26.647488
222.288064	7304.608737	26.652506
222.284004	7308.678055	26.657524
222.787517	7308.871644	26.662541
223.041321	7323.220548	26.667559
223.040104	7327.887401	26.672576
222.937737	7338.661929	26.677594
223.286392	7349.088397	26.682612
223.587250	7352.231031	26.687629
223.562562	7364.256041	26.692647
223.973620	7397.856275	26.697664
224.330772	7386.829512	26.702682
224.459009	7396.461052	26.707700
225.128478	7417.448302	26.712717
225.073520	7415.250849	26.717735
225.632898	7417.880981	26.722752
225.883993	7410.590421	26.727770
225.626198	7456.977848	26.732788
226.029703	7432.134887	26.737805
226.327127	7440.489224	26.742823
226.112606	7470.359081	26.747840
226.479154	7454.915105	26.752858
226.405960	7482.800117	26.757876
226.819754	7490.194887	26.762893
226.873201	7497.878429	26.767911
227.327108	7508.266201	26.772928
227.350347	7523.703255	26.777946
227.473100	7535.516062	26.782964
228.129415	7544.576474	26.787981
228.333601	7564.221019	26.792999
228.115986	7560.759071	26.798016
228.720044	7579.100636	26.803034
229.050367	7591.575174	26.808052
229.292391	7596.813132	26.813069
229.459639	7612.339053	26.818087
229.667250	7621.891206	26.823104
229.635204	7626.670076	26.828122
229.842596	7643.913584	26.833140
230.414360	7644.977557	26.838157
230.682979	7670.012809	26.843175
230.518394	7676.944362	26.848192
230.644370	7697.367929	26.853210
231.211370	7700.750690	26.858228
231.452800	7715.479630	26.863245
231.542104	7732.605155	26.868263
231.816261	7741.895776	26.873280
232.091851	7749.016068	26.878298
232.415543	7772.776688	26.883316
232.645185	7791.879670	26.888333
232.914925	7783.338811	26.893351
233.072194	7794.369709	26.898368
233.691288	7812.041925	26.903386
233.433555	7803.127978	26.908404
233.564878	7831.397283	26.913421
233.720620	7837.386354	26.918439
233.892445	7863.154963	26.923456
234.240751	7865.571755	26.928474
234.072074	7901.996685	26.933492
234.842631	7882.723585	26.938509
234.937406	7933.260421	26.943527
234.899108	7930.340268	26.948544
235.458759	7948.565836	26.953562
235.706115	7978.855656	26.958580
236.251446	7978.313182	26.963597
236.117250	8012.771262	26.968615
237.054282	7996.369466	26.973632
237.123772	8027.580030	26.978650
237.248266	8013.469225	26.983668
237.621108	8044.949360	26.988685
237.300982	8026.315750	26.993703
237.720474	8044.754983	26.998720
237.968165	8050.016592	27.003738
237.918661	8054.261745	27.008756
238.160690	8080.366544	27.013773
238.406964	8068.153063	27.018791
239.069099	8094.234199	27.023808
239.351886	8108.869595	27.028826
239.209872	8101.207802	27.033844
239.573214	8132.375680	27.038861
239.621850	8143.675948	27.043879
240.347425	8130.061729	27.048896
240.672555	8138.186215	27.053914
240.993505	8171.042454	27.058932
241.038479	8167.044356	27.063949
241.441621	8158.765291	27.068967
241.365081	8156.143115	27.073984
241.595467	8165.558222	27.079002
241.634172	8200.493556	27.084020
241.849327	8185.157154	27.089037
242.091279	8217.520921	27.094055
242.584773	8220.748707	27.099072
242.573455	8226.002878	27.104090
242.785158	8255.144612	27.109108
243.199789	8256.448497	27.114125
243.334742	8285.368037	27.119143
243.046575	8279.611638	27.124160
244.003158	8292.530669	27.129178
243.448640	8323.628075	27.134196
244.444447	8305.331234	27.139213
244.062944	8366.174768	27.144231
244.496294	8339.123088	27.149248
244.865887	8381.691481	27.154266
245.207259	8386.075077	27.159284
245.814202	8406.304135	27.164301
245.813387	8405.456839	27.169319
246.075217	8443.282777	27.174336
246.566816	8411.384748	27.179354
246.437225	8469.513172	27.184372
247.472830	8459.634127	27.189389
247.390893	8452.917845	27.194407
247.158095	8483.449684	27.199424
248.207955	8485.094564	27.204442
248.253339	8490.291791	27.209460
248.158955	8488.941638	27.214477
248.319195	8524.937957	27.219495
248.604582	8528.306787	27.224512
249.687781	8511.346057	27.229530
249.293645	8518.946453	27.234548
249.671148	8543.420511	27.239565
249.621078	8538.705663	27.244583
249.886662	8551.233032	27.249600
249.993604	8568.639198	27.254618
250.158212	8573.490107	27.259636
250.347341	8592.701690	27.264653
250.332609	8612.939630	27.269671
250.482547	8620.394338	27.274688
250.699774	8631.375775	27.279706
251.073849	8662.277084	27.284724
251.290387	8677.984721	27.289741
251.666726	8684.607829	27.294759
252.106275	8702.166514	27.299776
252.421094	8705.109706	27.304794
252.445872	8726.810627	27.309812
252.557536	8737.067323	27.314829
252.683761	8763.282270	27.319847
252.892278	8772.748068	27.324864
253.110421	8783.574847	27.329882
253.510941	8812.442456	27.334900
253.988644	8807.772450	27.339917
254.329970	8845.379783	27.344935
254.429195	8851.180761	27.349952
254.789668	8846.287064	27.354970
254.584709	8877.548265	27.359988
255.326136	8896.463285	27.365005
255.899428	8899.065509	27.370023
255.939211	8913.978469	27.375040
256.760872	8932.769401	27.380058
256.779132	8918.965043	27.385076
256.498912	8963.676356	27.390093
256.970895	8952.970087	27.395111
257.651217	8959.003870	27.400128
257.633258	8963.280056	27.405146
257.671989	8992.054200	27.410164
258.496251	8990.976211	27.415181
258.573267	8981.368444	27.420199
258.777185	9018.669977	27.425216
259.174380	9024.391265	27.430234
259.003401	9027.463497	27.435252
259.518494	9042.220954	27.440269
259.988938	9044.903731	27.445287
260.030276	9063.596510	27.450304
260.400080	9069.120339	27.455322
260.545895	9074.253367	27.460340
260.942215	9086.215807	27.465357
261.015697	9093.005015	27.470375
261.115627	9117.370024	27.475392
261.622480	9104.149019	27.480410
261.664405	9110.912968	27.485428
261.891994	9157.742161	27.490445
262.151660	9142.477165	27.495463
261.919347	9183.276436	27.500480
262.637633	9189.480926	27.505498
262.564352	9207.660198	27.510516
262.851987	9226.069979	27.515533
263.416511	9235.875542	27.520551
263.525260	9256.695089	27.525568
263.948556	9273.184467	27.530586
263.830864	9285.053905	27.535604
263.958256	9284.988784	27.540621
264.294400	9328.036181	27.545639
264.898315	9339.499878	27.550656
265.113079	9334.624922	27.555674
265.385015	9352.299619	27.560692
265.780894	9374.766241	27.565709
266.181727	9381.141024	27.570727
265.922100	9395.848796	27.575744
266.242096	9405.720202	27.580762
266.689525	9423.684144	27.585780
266.772884	9444.953008	27.590797
267.112109	9445.319987	27.595815
267.222893	9464.288246	27.600832
267.732803	9488.177735	27.605850
268.078012	9499.107542	27.610868
268.629739	9505.030237	27.615885
269.065239	9505.507389	27.620903
268.851813	9543.433503	27.625920
269.288354	9526.388602	27.630938
269.794832	9543.222289	27.635956
269.500458	9563.952670	27.640973
269.960284	9580.325214	27.645991
270.037151	9581.993899	27.651008
270.488198	9611.670268	27.656026
270.849305	9607.111069	27.661044
270.898430	9634.866099	27.666061
271.634475	9633.867057	27.671079
271.556503	9638.291896	27.676096
271.877509	9676.096572	27.681114
272.151585	9670.922066	27.686132
272.531090	9688.788949	27.691149
272.930195	9716.217246	27.696167
273.297430	9701.156064	27.701184
273.159195	9747.819162	27.706202
273.509940	9735.662830	27.711220
273.560715	9758.465973	27.716237
274.238738	9760.758133	27.721255
274.218158	9791.082925	27.726272
274.443019	9786.881809	27.731290
274.883572	9796.907782	27.736308
275.133927	9848.539038	27.741325
275.232187	9827.610993	27.746343
275.544259	9865.471869	27.751360
275.943799	9873.854193	27.756378
275.837886	9897.302246	27.761396
276.050584	9905.400372	27.766413
276.635268	9933.818989	27.771431
276.976964	9928.026482	27.776448
277.031084	9965.393201	27.781466
277.782919	9974.872717	27.786484
278.152792	9984.051905	27.791501
278.710843	9990.271652	27.796519
278.821858	10007.681203	27.801536
278.915645	10013.164781	27.806554
279.419396	10026.829182	27.811572
279.493873	10028.447146	27.816589
279.927166	10043.365797	27.821607
280.058315	10058.486863	27.826624
280.052715	10045.260542	27.831642
280.347600	10074.830509	27.836660
280.290318	10093.290822	27.841677
280.766501	10089.847155	27.846695
280.999805	10104.767050	27.851712
281.450581	10121.421003	27.856730
281.558957	10137.924936	27.861748
281.740037	10155.912537	27.866765
282.139959	10168.652798	27.871783
282.366668	10173.938575	27.876800
282.458976	10200.068580	27.881818
282.957469	10206.999101	27.886836
283.372548	10232.358035	27.891853
283.652142	10228.675738	27.896871
283.940714	10250.649249	27.901888
284.286430	10259.650666	27.906906
284.601279	10284.751797	27.911924
284.649532	10296.664444	27.916941
284.974231	10305.614937	27.921959
285.160297	10327.096905	27.926976
285.273575	10336.180272	27.931994
285.673258	10349.299261	27.937012
285.991311	10386.727269	27.942029
286.510945	10376.370085	27.947047
286.637276	10425.793189	27.952064
287.028765	10408.393645	27.957082
287.492252	10454.895746	27.962100
287.113657	10452.270940	27.967117
287.904638	10478.593457	27.972135
287.695456	10485.509406	27.977152
288.003999	10514.045538	27.982170
288.530053	10540.593756	27.987188
288.932748	10538.122614	27.992205
289.324921	10587.176491	27.997223
289.338943	10582.250495	28.002240
289.887813	10625.767451	28.007258
290.503377	10600.135458	28.012276
290.358139	10658.614831	28.017293
291.096594	10630.822185	28.022311
291.059612	10683.545656	28.027328
291.369925	10664.016951	28.032346
291.832038	10712.626457	28.037364
292.222479	10688.249645	28.042381
292.116266	10720.724289	28.047399
292.621218	10731.421380	28.052416
292.973734	10733.837982	28.057434
293.190510	10770.154532	28.062452
293.596228	10760.671892	28.067469
293.661643	10774.806241	28.072487
293.978134	10798.683398	28.077504
294.253726	10793.736500	28.082522
294.525956	10818.424664	28.087540
295.032746	10847.209612	28.092557
295.439073	10819.636005	28.097575
295.367143	10879.914657	28.102592
295.835758	10853.668181	28.107610
296.296929	10887.779837	28.112628
296.312369	10885.614331	28.117645
296.620442	10906.306810	28.122663
296.797168	10929.698045	28.127680
297.394048	10941.012603	28.132698
297.463495	10942.905741	28.137716
297.439004	10971.794095	28.142733
297.653981	10987.537853	28.147751
297.977368	11002.208181	28.152768
298.089403	11020.554105	28.157786
298.561131	11035.004070	28.162804
298.570617	11072.534315	28.167821
299.006493	11086.093239	28.172839
299.449798	11103.122127	28.177856
299.783917	11121.171884	28.182874
299.839921	11147.117286	28.187892
300.612226	11160.141004	28.192909
300.924630	11162.018272	28.197927
301.401561	11200.501200	28.202944
302.081821	11205.761888	28.207962
302.293053	11222.284066	28.212980
302.026307	11242.762073	28.217997
302.621549	11233.283957	28.223015
303.021030	11255.382139	28.228032
302.918371	11271.416465	28.233050
303.607310	11288.080589	28.238068
303.557106	11309.302150	28.243085
304.128071	11315.758082	28.248103
304.219832	11331.700493	28.253120
304.495344	11373.536831	28.258138
305.073205	11370.777529	28.263156
304.880309	11384.878062	28.268173
305.503764	11409.974782	28.273191
305.674767	11424.879552	28.278208
305.907438	11453.100184	28.283226
306.465271	11464.744835	28.288244
306.598385	11485.521873	28.293261
306.911875	11496.819055	28.298279
307.125857	11521.455871	28.303296
307.415840	11563.463185	28.308314
307.923758	11547.674135	28.313332
307.770921	11593.102925	28.318349
308.099908	11594.420774	28.323367
308.805244	11628.003686	28.328384
309.036070	11655.347436	28.333402
309.435953	11664.597644	28.338420
310.064887	11669.157943	28.343437
310.810476	11687.170351	28.348455
310.745906	11690.888853	28.353472
310.798960	11721.311255	28.358490
311.236694	11712.486404	28.363508
311.453857	11745.814852	28.368525
311.705183	11747.014835	28.373543
311.922803	11766.152352	28.378560
312.142942	11787.610116	28.383578
312.362088	11792.166500	28.388596
312.461443	11807.658402	28.393613
312.846224	11829.989983	28.398631
313.319815	11851.517634	28.403648
313.339911	11870.524236	28.408666
313.482762	11881.469540	28.413684
314.013813	11910.427383	28.418701
314.531446	11922.907176	28.423719
314.747897	11951.186024	28.428736
315.129745	11962.020495	28.433754
315.473246	11992.916026	28.438772
315.497218	12008.504756	28.443789
316.280431	12026.008248	28.448807
316.507632	12040.460568	28.453824
316.312652	12063.828975	28.458842
316.937024	12081.489285	28.463860
317.004824	12109.209688	28.468877
317.313939	12119.811479	28.473895
317.694442	12151.102251	28.478912
318.283311	12185.748820	28.483930
318.789448	12181.312735	28.488948
318.829464	12232.724960	28.493965
319.544070	12226.584087	28.498983
319.935398	12254.982619	28.504000
320.206780	12246.681798	28.509018
321.041036	12254.386986	28.514036
321.241908	12282.973732	28.519053
321.623968	12283.698192	28.524071
322.151813	12278.297006	28.529088
321.826167	12322.917678	28.534106
322.176804	12319.713322	28.539124
322.507995	12331.247188	28.544141
322.952278	12349.377082	28.549159
323.240463	12364.713922	28.554176
323.422899	12383.195302	28.559194
323.647016	12386.386666	28.564212
323.975862	12411.296865	28.569229
324.412486	12421.402363	28.574247
324.848425	12436.230688	28.579264
324.836513	12457.103207	28.584282
325.333333	12468.049788	28.589300
325.586741	12490.680928	28.594317
326.016921	12511.785115	28.599335
326.381070	12516.352259	28.604352
326.313096	12538.714735	28.609370
326.752323	12552.252805	28.614388
327.089243	12572.307003	28.619405
327.304090	12589.552259	28.624423
327.747662	12608.783919	28.629440
327.850614	12638.480806	28.634458
328.412666	12658.607074	28.639476
328.724972	12701.235008	28.644493
328.955708	12699.319076	28.649511
329.289159	12718.501324	28.654528
329.294671	12749.793274	28.659546
329.851373	12752.263270	28.664564
330.370688	12763.518763	28.669581
330.222230	12793.689318	28.674599
330.784649	12814.503074	28.679616
331.080509	12815.784205	28.684634
331.242536	12827.161424	28.689652
331.444261	12876.572849	28.694669
331.927818	12885.563127	28.699687
332.252745	12904.172182	28.704704
332.557429	12925.227679	28.709722
333.140770	12929.084089	28.714740
333.488075	12965.339851	28.719757
333.814598	13007.310714	28.724775
334.146943	13003.642766	28.729792
334.500895	13021.240029	28.734810
335.330158	13037.879997	28.739828
335.291567	13070.948091	28.744845
335.476014	13071.683423	28.749863
336.073005	13085.561660	28.754880
336.130755	13112.573941	28.759898
336.767136	13135.506499	28.764916
337.058734	13144.493873	28.769933
337.186153	13167.817713	28.774951
337.836988	13188.495891	28.779968
338.008173	13206.874593	28.784986
338.495639	13219.799094	28.790004
338.680831	13229.230098	28.795021
339.210018	13268.541957	28.800039
339.541068	13272.993587	28.805056
339.437837	13289.855439	28.810074
340.109200	13305.222888	28.815092
340.468591	13330.561472	28.820109
340.643431	13336.045150	28.825127
340.741532	13362.063789	28.830144
341.263950	13401.825542	28.835162
341.802953	13388.232244	28.840180
341.750807	13433.245902	28.845197
342.185589	13447.462422	28.850215
342.621138	13480.158702	28.855232
343.071982	13495.818881	28.860250
343.332533	13511.366534	28.865268
343.431816	13525.779063	28.870285
343.761107	13579.554366	28.875303
344.311017	13580.136832	28.880320
344.437209	13605.331697	28.885338
345.059436	13623.998163	28.890356
345.371918	13646.787701	28.895373
345.672986	13677.052294	28.900391
346.689249	13684.187467	28.905408
346.585091	13695.081544	28.910426
346.997178	13706.886551	28.915444
347.400495	13731.983250	28.920461
347.564211	13761.700590	28.925479
348.050457	13760.571604	28.930496
348.438587	13779.224204	28.935514
348.945769	13793.023340	28.940532
349.373593	13790.816993	28.945549
349.483134	13795.832652	28.950567
349.728662	13826.797222	28.955584
349.564199	13828.407328	28.960602
349.677697	13855.659900	28.965620
350.102969	13892.919409	28.970637
350.547498	13915.734752	28.975655
351.120073	13921.298427	28.980672
351.169650	13963.161898	28.985690
351.574479	13987.216669	28.990708
351.818387	14003.456740	28.995725
351.784568	14026.836124	29.000743
352.350388	14069.649576	29.005760
352.863175	14092.164725	29.010778
352.971924	14103.295165	29.015796
353.770532	14149.380329	29.020813
353.876424	14177.116043	29.025831
354.359183	14182.534921	29.030848
355.005557	14230.975124	29.035866
355.754000	14237.702879	29.040884
355.829938	14253.133309	29.045901
356.190784	14276.336240	29.050919
356.818346	14288.235085	29.055936
356.577329	14329.716237	29.060954
357.192240	14331.325297	29.065972
357.853744	14359.318970	29.070989
358.160054	14371.868317	29.076007
358.687605	14388.008596	29.081024
359.060247	14401.944753	29.086042
359.652286	14433.316236	29.091060
360.261523	14432.497243	29.096077
360.068085	14438.707049	29.101095
360.668578	14464.641019	29.106112
360.746692	14481.690093	29.111130
361.040614	14499.516786	29.116148
361.439697	14511.456052	29.121165
361.479579	14533.647515	29.126183
362.180972	14550.340230	29.131200
362.211628	14569.323525	29.136218
362.573070	14607.611322	29.141236
362.958723	14621.492864	29.146253
363.133439	14628.440236	29.151271
363.661162	14675.041097	29.156288
364.414653	14692.610186	29.161306
364.603492	14696.574203	29.166324
364.885883	14723.293369	29.171341
365.060716	14747.252952	29.176359
365.469658	14760.233496	29.181376
365.780203	14793.401985	29.186394
366.203102	14812.247016	29.191412
366.631610	14828.733483	29.196429
366.305904	14867.150611	29.201447
366.901569	14878.348482	29.206464
367.598282	14893.586175	29.211482
367.836435	14921.050452	29.216500
368.335440	14930.170069	29.221517
368.561088	14961.853029	29.226535
369.128974	14977.100314	29.231552
369.144454	15003.121137	29.236570
369.439741	15022.593313	29.241588
369.987725	15027.488248	29.246605
370.215816	15080.027279	29.251623
370.794794	15084.618346	29.256640
371.266714	15102.874954	29.261658
371.442879	15134.651964	29.266676
371.847016	15170.902736	29.271693
372.143397	15172.767723	29.276711
372.387212	15216.221988	29.281728
372.792573	15239.575064	29.286746
373.366732	15252.712143	29.291764
373.752531	15290.978088	29.296781
374.238293	15294.417000	29.301799
374.501412	15328.271545	29.306816
375.100454	15347.916652	29.311834
375.296151	15358.703120	29.316852
375.734927	15368.273056	29.321869
375.915281	15421.950944	29.326887
376.575675	15424.766809	29.331904
377.050950	15444.112241	29.336922
377.328402	15467.308917	29.341940
378.113770	15498.089889	29.346957
378.488279	15515.425299	29.351975
378.519203	15518.049513	29.356992
379.131596	15542.050734	29.362010
379.303061	15571.144593	29.367028
379.729013	15594.027699	29.372045
380.026097	15607.132477	29.377063
380.146635	15627.448562	29.382080
380.631962	15634.038593	29.387098
380.929634	15685.544201	29.392116
381.456166	15700.917872	29.397133
381.864394	15719.972326	29.402151
382.230399	15763.713733	29.407168
382.543456	15784.548168	29.412186
383.210509	15811.706374	29.417204
383.435706	15822.015226	29.422221
383.413389	15847.603621	29.427239
384.113439	15871.429216	29.432256
384.490996	15898.906295	29.437274
384.714879	15928.398214	29.442292
385.335143	15935.608891	29.447309
385.561046	15963.269768	29.452327
385.701295	15986.881249	29.457344
386.381578	16003.841283	29.462362
386.019193	16058.471310	29.467380
386.830941	16062.872760	29.472397
387.431995	16099.204766	29.477415
387.989673	16118.997395	29.482432
388.228204	16129.989948	29.487450
388.109644	16161.429096	29.492468
389.192660	16175.987134	29.497485
389.212156	16205.754043	29.502503
389.391945	16245.589011	29.507520
390.128222	16247.727691	29.512538
390.558868	16281.972642	29.517556
390.680964	16297.488509	29.522573
391.172295	16324.512163	29.527591
391.666555	16344.644865	29.532608
391.948819	16367.967806	29.537626
391.989995	16396.813651	29.542644
392.676687	16433.583920	29.547661
393.052354	16450.457572	29.552679
393.478081	16467.614367	29.557696
394.058534	16487.320193	29.562714
394.058824	16526.544024	29.567732
394.678155	16540.148871	29.572749
395.349771	16566.630121	29.577767
395.909788	16582.932884	29.582784
396.207994	16614.043198	29.587802
396.100119	16641.562242	29.592820
396.582677	16642.618518	29.597837
396.906475	16677.931243	29.602855
397.361347	16722.167747	29.607872
398.007905	16746.117190	29.612890
398.414017	16774.599333	29.617908
398.852593	16790.734287	29.622925
398.924795	16813.096213	29.627943
399.692625	16878.024626	29.632960
400.008766	16867.240056	29.637978
400.432667	16914.213828	29.642996
401.087917	16928.700406	29.648013
401.242902	16954.572196	29.653031
401.088424	16985.160173	29.658048
401.556862	17006.409355	29.663066
402.099397	17028.366569	29.668084
402.501982	17060.985606	29.673101
402.992741	17104.911221	29.678119
403.815063	17116.787552	29.683136
404.038221	17136.381668	29.688154
404.272401	17168.749051	29.693172
404.679793	17201.464854	29.698189
404.951146	17232.769653	29.703207
405.378404	17252.580982	29.708224
406.076143	17282.549159	29.713242
406.522198	17309.497119	29.718260
407.296712	17333.671362	29.723277
407.380593	17361.679202	29.728295
408.023692	17374.984572	29.733312
408.644692	17386.164311	29.738330
408.594243	17417.534535	29.743348
409.127882	17419.859997	29.748365
409.789862	17441.411202	29.753383
409.574740	17464.399136	29.758400
410.172656	17484.778411	29.763418
410.324760	17519.944446	29.768436
410.909094	17541.258966	29.773453
411.081898	17558.571640	29.778471
411.362078	17582.666384	29.783488
412.082766	17603.703968	29.788506
412.073592	17643.763385	29.793524
412.400461	17657.295751	29.798541
412.936618	17690.215880	29.803559
412.988079	17723.141653	29.808576
413.687181	17752.337736	29.813594
414.115904	17788.394706	29.818612
414.616596	17819.798399	29.823629
415.083334	17842.473344	29.828647
415.780728	17874.275315	29.833664
416.268988	17883.997501	29.838682
416.299526	17936.347045	29.843700
416.860858	17952.027851	29.848717
417.574394	17976.581308	29.853735
417.942755	17993.586551	29.858752
418.622971	18019.508324	29.863770
418.693998	18051.039996	29.868788
419.394652	18069.338002	29.873805
419.704589	18095.043316	29.878823
420.144365	18113.157354	29.883840
420.954642	18131.170654	29.888858
421.065463	18152.764605	29.893876
421.578078	18168.601422	29.898893
422.243825	18196.826523	29.903911
422.562578	18219.011044	29.908928
422.687854	18228.531051	29.913946
423.091666	18256.938935	29.918964
423.570006	18279.277247	29.923981
423.994418	18308.409488	29.928999
424.001382	18319.108221	29.934016
424.382250	18366.318846	29.939034
424.780752	18392.954230	29.944052
425.286366	18426.790623	29.949069
425.720484	18443.682736	29.954087
425.851877	18484.470541	29.959104
426.359994	18523.117734	29.964122
426.475868	18557.943667	29.969140
427.135049	18590.016191	29.974157
427.647730	18620.529442	29.979175
428.130603	18658.135323	29.984192
428.752180	18682.100614	29.989210
429.066856	18723.999223	29.994228
429.310219	18753.582407	29.999245
430.031324	18771.687829	30.004263
430.293922	18811.434710	30.009280
430.793228	18838.895756	30.014298
431.482620	18874.358990	30.019316
432.131204	18893.049741	30.024333
432.608114	18921.292862	30.029351
432.801389	18951.854109	30.034368
433.036115	18962.602039	30.039386
433.547550	18986.441251	30.044404
433.996432	19001.888279	30.049421
434.341244	19025.169436	30.054439
434.862855	19045.881443	30.059456
435.016410	19076.444538	30.064474
435.574762	19097.995670	30.069492
435.958551	19116.272170	30.074509
436.615861	19161.082427	30.079527
436.631211	19177.500306	30.084544
437.274171	19186.327378	30.089562
437.950688	19240.124121	30.094580
438.356639	19256.769237	30.099597
438.294035	19272.153921	30.104615
438.690946	19323.378455	30.109632
439.618947	19320.428157	30.114650
439.733475	19390.480669	30.119668
440.010384	19392.607963	30.124685
440.837066	19431.406674	30.129703
441.078515	19468.839975	30.134720
441.977141	19495.683810	30.139738
442.285999	19521.883811	30.144756
442.683777	19536.193382	30.149773
442.867865	19575.786601	30.154791
443.502487	19598.524384	30.159808
444.141827	19639.913074	30.164826
444.599092	19653.771515	30.169844
445.146923	19679.043886	30.174861
445.284836	19703.846919	30.179879
445.524176	19748.174235	30.184896
445.847849	19767.909610	30.189914
446.373895	19793.032869	30.194932
447.026106	19828.455382	30.199949
447.456361	19853.771178	30.204967
447.838034	19887.593880	30.209984
448.277367	19920.042393	30.215002
448.826163	19969.674641	30.220020
448.923219	19986.368961	30.225037
449.419794	20010.712550	30.230055
449.785603	20059.981288	30.235072
450.224546	20084.433002	30.240090
450.910391	20131.576768	30.245108
451.398216	20160.591342	30.250125
451.723810	20183.581987	30.255143
452.037365	20221.129632	30.260160
452.919318	20263.527499	30.265178
453.816807	20284.851033	30.270196
454.476620	20298.987659	30.275213
454.851523	20329.588030	30.280231
454.717957	20354.203034	30.285248
455.442144	20385.058929	30.290266
456.050373	20412.256159	30.295284
456.148851	20439.090891	30.300301
456.742713	20452.436888	30.305319
456.731717	20480.523529	30.310336
457.456355	20505.800180	30.315354
457.760274	20545.685464	30.320372
458.328659	20562.017087	30.325389
458.801146	20586.059468	30.330407
458.828500	20617.467046	30.335424
459.452982	20644.634136	30.340442
459.841024	20670.092252	30.345460
460.373746	20707.302959	30.350477
460.977525	20733.907678	30.355495
461.219561	20770.514754	30.360512
461.788706	20793.090674	30.365530
462.275142	20820.588766	30.370548
462.715542	20849.043196	30.375565
463.706595	20872.450179	30.380583
463.813569	20917.135405	30.385600
464.576172	20934.094451	30.390618
465.058097	20954.929907	30.395636
465.307582	20991.320925	30.400653
465.767095	21022.774660	30.405671
465.998065	21042.993023	30.410688
466.383309	21071.492083	30.415706
467.031693	21105.502919	30.420724
467.415655	21138.408522	30.425741
468.156756	21160.948524	30.430759
468.020217	21191.278453	30.435776
468.430758	21234.289574	30.440794
469.329181	21272.795564	30.445812
469.787815	21308.060899	30.450829
470.692893	21319.297471	30.455847
470.536797	21370.655786	30.460864
471.245654	21388.019234	30.465882
471.549336	21423.404017	30.470900
472.386295	21442.035540	30.475917
472.760079	21474.415027	30.480935
473.044831	21518.829109	30.485952
473.410915	21538.305192	30.490970
474.247508	21582.084199	30.495988
474.557131	21614.621467	30.501005
475.411755	21632.320303	30.506023
475.457814	21674.714184	30.511040
475.763412	21709.667725	30.516058
476.331470	21740.133761	30.521076
476.947886	21772.283833	30.526093
477.786094	21801.364950	30.531111
478.002826	21835.817862	30.536128
478.569190	21861.494439	30.541146
479.244357	21884.509864	30.546164
479.637771	21919.125405	30.551181
479.833801	21941.944741	30.556199
480.190463	21964.669216	30.561216
480.679739	21991.660140	30.566234
481.381272	22034.951578	30.571252
481.622378	22074.262037	30.576269
482.200225	22089.936520	30.581287
482.608952	22121.024872	30.586304
482.921240	22149.557199	30.591322
483.420414	22177.542367	30.596340
483.821058	22218.426561	30.601357
484.780118	22242.636946	30.606375
485.222339	22273.369788	30.611392
485.614689	22282.593757	30.616410
486.004029	22330.785698	30.621428
486.279595	22360.905736	30.626445
487.094705	22373.468743	30.631463
487.701396	22404.460750	30.636480
487.895680	22438.547600	30.641498
488.368235	22456.513795	30.646516
488.676185	22499.014665	30.651533
488.992896	22539.301098	30.656551
489.613357	22575.248398	30.661568
490.154125	22595.548575	30.666586
490.481204	22632.420128	30.671604
490.938829	22676.708335	30.676621
491.608942	22707.482907	30.681639
491.968508	22735.689783	30.686656
491.949396	22800.654205	30.691674
493.119784	22823.034492	30.696692
493.593929	22887.775779	30.701709
494.106651	22876.865209	30.706727
494.783496	22926.959371	30.711744
495.047173	22977.579477	30.716762
495.826765	22993.660646	30.721780
495.968954	23045.258068	30.726797
496.789930	23077.293160	30.731815
496.978412	23107.905795	30.736832
497.533939	23139.072010	30.741850
497.934189	23180.625093	30.746868
498.473106	23232.049661	30.751885
499.322405	23250.689251	30.756903
499.621857	23280.302362	30.761920
499.968692	23340.122575	30.766938
500.847401	23360.915742	30.771956
501.050516	23391.488000	30.776973
501.818527	23444.835632	30.781991
502.703448	23468.525695	30.787008
503.179829	23486.924875	30.792026
503.872243	23519.648480	30.797044
503.874522	23552.206406	30.802061
504.491158	23579.315237	30.807079
504.972978	23603.001975	30.812096
505.430034	23653.152351	30.817114
506.202148	23658.539047	30.822132
506.450386	23695.724157	30.827149
506.795473	23720.126775	30.832167
507.093614	23778.790665	30.837184
507.453330	23795.779971	30.842202
507.922256	23848.852087	30.847220
508.756781	23877.683215	30.852237
509.409580	23906.569336	30.857255
509.525322	23944.190445	30.862272
510.211951	23970.985547	30.867290
510.465435	24000.234758	30.872308
511.067685	24052.877518	30.877325
511.823547	24074.337877	30.882343
512.282458	24105.739573	30.887360
512.689497	24129.706820	30.892378
513.249130	24170.736936	30.897396
513.512075	24217.615695	30.902413
514.072297	24219.659545	30.907431
514.543001	24290.971657	30.912448
514.977630	24310.017258	30.917466
515.417794	24352.635158	30.922484
516.242261	24382.032793	30.927501
516.584791	24431.246824	30.932519
517.537101	24447.627288	30.937536
517.581367	24494.002911	30.942554
518.370514	24546.210298	30.947572
518.856473	24566.165700	30.952589
519.280209	24599.281707	30.957607
519.732373	24645.866134	30.962624
520.263700	24674.524088	30.967642
521.240047	24706.149395	30.972660
521.625455	24759.248093	30.977677
522.037599	24792.735786	30.982695
522.594626	24816.883409	30.987712
522.871179	24853.010393	30.992730
523.405905	24899.891983	30.997748
523.613374	24937.447263	31.002765
524.440980	24976.921207	31.007783
525.250138	25017.311944	31.012800
525.524973	25054.822110	31.017818
526.247088	25093.130772	31.022836
526.675319	25150.203542	31.027853
527.161656	25173.323165	31.032871
527.868265	25222.847156	31.037888
528.246023	25255.612645	31.042906
528.674722	25282.486494	31.047924
529.443758	25338.231886	31.052941
529.977064	25377.475627	31.057959
530.105875	25401.474927	31.062976
530.553232	25454.174563	31.067994
531.383562	25496.965763	31.073012
531.384228	25538.120730	31.078029
532.139016	25582.290933	31.083047
532.917569	25624.879606	31.088064
533.438897	25666.314339	31.093082
533.941352	25709.305641	31.098100
534.803860	25750.088344	31.103117
535.355901	25792.942781	31.108135
536.048866	25825.104651	31.113152
536.611501	25859.291414	31.118170
536.969703	25879.931322	31.123188
537.397399	25956.313596	31.128205
537.591393	25965.153797	31.133223
538.153215	26007.957622	31.138240
538.478101	26020.080129	31.143258
538.704421	26080.743590	31.148276
539.631331	26117.424487	31.153293
540.254916	26163.777277	31.158311
540.610676	26195.509904	31.163328
541.045712	26262.021586	31.168346
541.986267	26268.219779	31.173364
542.200940	26344.082440	31.178381
542.618702	26355.641322	31.183399
543.398436	26403.916560	31.188416
543.752637	26452.777299	31.193434
544.505467	26497.570336	31.198452
545.048240	26533.635079	31.203469
545.833887	26556.992642	31.208487
546.555414	26614.811716	31.213504
546.759473	26646.533947	31.218522
547.391826	26678.426730	31.223540
547.932884	26717.108455	31.228557
548.319218	26783.689927	31.233575
549.396718	26818.518369	31.238592
549.343807	26860.947331	31.243610
549.972892	26885.519119	31.248628
550.490101	26972.646418	31.253645
551.137049	26997.209230	31.258663
551.597169	27041.756549	31.263680
552.113642	27093.128599	31.268698
553.000036	27134.795754	31.273716
553.324882	27187.606470	31.278733
553.981002	27220.423820	31.283751
555.016712	27251.026061	31.288768
555.150467	27308.147896	31.293786
555.845155	27353.850714	31.298804
556.321388	27380.158786	31.303821
556.830756	27421.426635	31.308839
557.714867	27457.998457	31.313856
558.067218	27523.252220	31.318874
558.525716	27537.101248	31.323892
559.301100	27571.219173	31.328909
559.597640	27637.437945	31.333927
560.344991	27673.467150	31.338944
561.053936	27718.515604	31.343962
561.723178	27743.807925	31.348980
562.338012	27790.065957	31.353997
562.726842	27819.742579	31.359015
563.169008	27855.904310	31.364032
563.597240	27921.786555	31.369050
564.190452	27947.951654	31.374068
564.601640	27997.860593	31.379085
565.187677	28027.525098	31.384103
565.754070	28093.107131	31.389120
566.542606	28138.104688	31.394138
567.190584	28174.757505	31.399156
567.708099	28200.062103	31.404173
567.998624	28259.444027	31.409191
568.968934	28283.568883	31.414208
569.114579	28320.245305	31.419226
569.731706	28359.397894	31.424244
570.290885	28384.299051	31.429261
570.724889	28429.180548	31.434279
571.665051	28457.210517	31.439296
571.828104	28500.715585	31.444314
572.922854	28540.455954	31.449332
573.033907	28565.613126	31.454349
573.706035	28624.746522	31.459367
574.265733	28647.659347	31.464384
574.465262	28709.681120	31.469402
575.141625	28751.344938	31.474420
575.665741	28782.683172	31.479437
575.961638	28842.564335	31.484455
576.374868	28885.753250	31.489472
576.877457	28939.878469	31.494490
577.621761	28985.602433	31.499508
577.955911	29044.096242	31.504525
578.677103	29100.254682	31.509543
579.476235	29152.688205	31.514560
579.850879	29217.468552	31.519578
580.644273	29254.012409	31.524596
581.585876	29300.878280	31.529613
582.177598	29349.104824	31.534631
582.994099	29405.999257	31.539648
583.038755	29450.611501	31.544666
583.625013	29496.061081	31.549684
584.635050	29546.259208	31.554701
585.009152	29604.507561	31.559719
585.889636	29640.729547	31.564736
586.007857	29685.789305	31.569754
586.967802	29731.979016	31.574772
587.629337	29790.065641	31.579789
588.048560	29829.154018	31.584807
588.825413	29869.934802	31.589824
589.603449	29924.917711	31.594842
590.222307	29960.373627	31.599860
590.971690	30005.902666	31.604877
591.199316	30051.226528	31.609895
592.126679	30074.287693	31.614912
592.694630	30127.864338	31.619930
593.102289	30182.040330	31.624948
593.938708	30217.474768	31.629965
594.381913	30251.005112	31.634983
594.631182	30291.833150	31.640000
595.358827	30337.134913	31.645018
595.774402	30387.939344	31.650036
596.276804	30457.230456	31.655053
596.688313	30493.294208	31.660071
597.677581	30543.145703	31.665088
598.133503	30599.244397	31.670106
598.372497	30640.894457	31.675124
599.582786	30690.408616	31.680141
599.785620	30745.035157	31.685159
600.781733	30793.162181	31.690176
601.078521	30821.046543	31.695194
601.703650	30860.618381	31.700212
602.259602	30898.007516	31.705229
602.700363	30953.734749	31.710247
603.792625	30989.046596	31.715264
604.058814	31043.626220	31.720282
604.432254	31091.903717	31.725300
605.372358	31120.404816	31.730317
605.606708	31180.184587	31.735335
605.905631	31225.760398	31.740352
606.777003	31277.243633	31.745370
607.331940	31316.205211	31.750388
608.011463	31375.495572	31.755405
608.532155	31414.694519	31.760423
609.259249	31478.174740	31.765440
609.770821	31532.430071	31.770458
610.252172	31575.900535	31.775476
611.325979	31636.813885	31.780493
611.450547	31699.361726	31.785511
612.409039	31741.902406	31.790528
612.722343	31787.855752	31.795546
613.808999	31855.165267	31.800564
614.633629	31895.142845	31.805581
614.876560	31943.180420	31.810599
615.822432	31992.583024	31.815616
616.353196	32052.243114	31.820634
616.969659	32097.682518	31.825652
617.579019	32137.898289	31.830669
618.124218	32173.239921	31.835687
618.863028	32258.418436	31.840704
619.667636	32283.270722	31.845722
619.743156	32341.426629	31.850740
620.844498	32380.426667	31.855757
621.425805	32438.574880	31.860775
622.324008	32484.014621	31.865792
622.899644	32534.775000	31.870810
623.374030	32579.035739	31.875828
624.102494	32611.053343	31.880845
624.542990	32670.998003	31.885863
625.176120	32719.539983	31.890880
625.889429	32772.076029	31.895898
625.998472	32824.960656	31.900916
626.850542	32861.619893	31.905933
627.123134	32929.953997	31.910951
628.115101	32961.323483	31.915968
628.874807	33029.697074	31.920986
629.494531	33096.126107	31.926004
630.169325	33128.326649	31.931021
630.362842	33181.164288	31.936039
631.270195	33239.901785	31.941056
631.791086	33293.712210	31.946074
632.289392	33328.849421	31.951092
633.383855	33395.664330	31.956109
633.924773	33454.820327	31.961127
634.421707	33477.286515	31.966144
635.131924	33522.286178	31.971162
635.480567	33573.839356	31.976180
636.085972	33618.956853	31.981197
636.387964	33667.384113	31.986215
637.427519	33716.568909	31.991232
638.164570	33762.767661	31.996250
638.787799	33815.346593	32.001268
639.723384	33851.086789	32.006285
640.266719	33915.236186	32.011303
640.698106	33948.474890	32.016320
641.652599	33993.726982	32.021338
641.602870	34047.299694	32.026356
642.477353	34091.992592	32.031373
642.981501	34140.488353	32.036391
643.859509	34198.308627	32.041408
644.438864	34250.971592	32.046426
644.793236	34304.958420	32.051444
646.028540	34361.547997	32.056461
646.537606	34411.227604	32.061479
646.911448	34452.949376	32.066496
647.809932	34506.854952	32.071514
648.316811	34554.938484	32.076532
648.483894	34613.426708	32.081549
649.407987	34671.611742	32.086567
650.227693	34725.562100	32.091584
650.937216	34786.518301	32.096602
651.560052	34845.943663	32.101620
652.586327	34885.913731	32.106637
652.856514	34957.987906	32.111655
653.666914	34992.853530	32.116672
654.293888	35050.951631	32.121690
654.964352	35115.756976	32.126708
655.500305	35169.049295	32.131725
656.199445	35224.866463	32.136743
656.613974	35273.890565	32.141760
657.475256	35335.054772	32.146778
657.918211	35389.002637	32.151796
659.136528	35462.915927	32.156813
659.674061	35507.691514	32.161831
660.390958	35558.788643	32.166848
660.841157	35599.315633	32.171866
661.323382	35668.839928	32.176884
662.469112	35712.511863	32.181901
662.931374	35781.530605	32.186919
663.578261	35836.603007	32.191936
664.208983	35885.411611	32.196954
664.541451	35948.068496	32.201972
665.709170	36001.534043	32.206989
665.909419	36066.417949	32.212007
666.689955	36125.742362	32.217024
667.776590	36181.502612	32.222042
668.115003	36230.246832	32.227060
668.931616	36286.611668	32.232077
669.155783	36353.413090	32.237095
670.178595	36390.235833	32.242112
670.863604	36433.136411	32.247130
671.841946	36485.676701	32.252148
672.937198	36508.761180	32.257165
673.351524	36550.797065	32.262183
674.073365	36601.909212	32.267200
674.781271	36628.607516	32.272218
674.911800	36674.865209	32.277236
675.647280	36745.934953	32.282253
675.966709	36771.790386	32.287271
676.709252	36851.858544	32.292288
677.687804	36878.307624	32.297306
677.809131	36940.971883	32.302324
678.731890	36986.744837	32.307341
678.973300	37056.986444	32.312359
679.594271	37102.229150	32.317376
680.409400	37179.419469	32.322394
680.906550	37242.452277	32.327412
681.889395	37307.979466	32.332429
682.547665	37350.881923	32.337447
683.611786	37418.813577	32.342464
684.585000	37468.199768	32.347482
684.524572	37526.898365	32.352500
685.505538	37596.548330	32.357517
686.251704	37642.910903	32.362535
686.898878	37697.737112	32.367552
687.471070	37778.796995	32.372570
688.053825	37830.319735	32.377588
688.983247	37894.419790	32.382605
689.112632	37975.666216	32.387623
690.370763	38018.031822	32.392640
691.184695	38087.300473	32.397658
691.531646	38145.364020	32.402676
692.083940	38208.607672	32.407693
693.260926	38280.425615	32.412711
693.750784	38337.358639	32.417728
694.833348	38408.263471	32.422746
695.283947	38459.457563	32.427764
695.685597	38519.587090	32.432781
696.824438	38587.713388	32.437799
697.241960	38623.801736	32.442816
697.843093	38716.475838	32.447834
698.610008	38759.823423	32.452852
699.217486	38844.126196	32.457869
700.176255	38882.353746	32.462887
700.720293	38985.244853	32.467904
701.619768	39011.169056	32.472922
702.398955	39111.041793	32.477940
703.245764	39133.081467	32.482957
703.891393	39224.850917	32.487975
704.674077	39246.825262	32.492992
705.519338	39318.008212	32.498010
705.593626	39364.605473	32.503028
707.021058	39422.734754	32.508045
707.806461	39467.699031	32.513063
708.166146	39528.701345	32.518080
708.491733	39571.205131	32.523098
709.345907	39611.690091	32.528116
709.593357	39686.424614	32.533133
710.497941	39705.934464	32.538151
711.078043	39814.575623	32.543168
711.858882	39840.644560	32.548186
712.228452	39927.308575	32.553204
713.184024	39961.915433	32.558221
714.178459	40038.588824	32.563239
714.508682	40103.637854	32.568256
715.433852	40142.480703	32.573274
716.053182	40236.038530	32.578292
716.671057	40277.642873	32.583309
717.162224	40347.511451	32.588327
717.713290	40427.568684	32.593344
718.925628	40479.434484	32.598362
719.525865	40541.628975	32.603380
720.084691	40639.491039	32.608397
721.318560	40690.776899	32.613415
721.732855	40741.731342	32.618432
722.578760	40834.277099	32.623450
723.142280	40878.269606	32.628468
724.087164	40948.893165	32.633485
724.821998	41007.858810	32.638503
725.541256	41117.514298	32.643520
726.134207	41151.403858	32.648538
727.057265	41191.116779	32.653556
727.656657	41275.582698	32.658573
728.859118	41365.951941	32.663591
728.827520	41412.967478	32.668608
730.298691	41472.943490	32.673626
730.574112	41541.074003	32.678644
731.506707	41602.088724	32.683661
732.388328	41688.640734	32.688679
732.971042	41730.705248	32.693696
733.853654	41788.684915	32.698714
734.128850	41900.261242	32.703732
734.810845	41931.034538	32.708749
736.148679	42020.776945	32.713767
736.627828	42062.193239	32.718784
737.044349	42148.023611	32.723802
738.157921	42209.465884	32.728820
738.793081	42275.529692	32.733837
739.489545	42360.755120	32.738855
740.525279	42431.818230	32.743872
741.196414	42474.173295	32.748890
741.875138	42561.673571	32.753908
742.612027	42606.608111	32.758925
743.502797	42670.803296	32.763943
744.073102	42740.367806	32.768960
745.150999	42812.864120	32.773978
745.669408	42869.955982	32.778996
746.185017	42930.063980	32.784013
747.274894	43006.599848	32.789031
747.851279	43054.668098	32.794048
748.722563	43126.280718	32.799066
749.269660	43180.564848	32.804084
749.813245	43235.247156	32.809101
750.719684	43294.250121	32.814119
751.078000	43350.142013	32.819136
751.829907	43410.576822	32.824154
752.435734	43478.097772	32.829172
753.256906	43562.889760	32.834189
754.358229	43617.254224	32.839207
754.781832	43693.684701	32.844224
755.911936	43750.022829	32.849242
756.721609	43810.405680	32.854260
757.304123	43875.114969	32.859277
758.129976	43931.931128	32.864295
759.115737	44008.759301	32.869312
759.760610	44067.664594	32.874330
760.796705	44119.968522	32.879348
760.952546	44215.468759	32.884365
762.030177	44254.113710	32.889383
762.944056	44347.544510	32.894400
763.692171	44407.677418	32.899418
764.603615	44470.336582	32.904436
765.037254	44520.535729	32.909453
766.203880	44609.113821	32.914471
766.665175	44650.668511	32.919488
767.646769	44711.749545	32.924506
768.119742	44795.962609	32.929524
768.853568	44848.237986	32.934541
770.213125	44927.799434	32.939559
770.957209	44985.486976	32.944576
771.675173	45042.118898	32.949594
772.218749	45115.441807	32.954612
773.006339	45182.353691	32.959629
774.052359	45254.272236	32.964647
774.229655	45327.152739	32.969664
775.332552	45372.023594	32.974682
775.920359	45451.019395	32.979700
776.690354	45528.617388	32.984717
777.920621	45598.526838	32.989735
778.270165	45661.680395	32.994752
779.268249	45720.083937	32.999770
779.883842	45814.895114	33.004788
780.848143	45872.777691	33.009805
781.401299	45946.430671	33.014823
782.012848	46010.436604	33.019840
782.544334	46094.760201	33.024858
783.361277	46164.103582	33.029876
783.798984	46232.876623	33.034893
785.074007	46318.837070	33.039911
785.845851	46403.575048	33.044928
786.594117	46471.084951	33.049946
787.489989	46535.426141	33.054964
788.049869	46642.047001	33.059981
789.174376	46692.546272	33.064999
789.874232	46752.142834	33.070016
790.525313	46832.683902	33.075034
791.293259	46901.211393	33.080052
791.895212	46953.968393	33.085069
793.065017	47015.948811	33.090087
793.267205	47094.275132	33.095104
794.059186	47163.364575	33.100122
795.056927	47231.105876	33.105140
795.351188	47326.367605	33.110157
796.778503	47383.774481	33.115175
797.409257	47453.291423	33.120192
797.985904	47541.971992	33.125210
798.842469	47611.797528	33.130228
799.568620	47679.678441	33.135245
800.408319	47762.758884	33.140263
801.208856	47850.982582	33.145280
802.126993	47924.866585	33.150298
803.199219	48009.195344	33.155316
803.891954	48083.399856	33.160333
804.932771	48152.516684	33.165351
805.506662	48229.416362	33.170368
806.364525	48310.906255	33.175386
807.152702	48387.122531	33.180404
807.863340	48471.192368	33.185421
808.626172	48539.013957	33.190439
809.540968	48629.132317	33.195456
810.605670	48699.089954	33.200474
811.578697	48753.973622	33.205492
812.173284	48858.696546	33.210509
813.287764	48925.952484	33.215527
813.710419	49000.456263	33.220544
814.767928	49092.453810	33.225562
815.847418	49157.321249	33.230580
816.223988	49228.980832	33.235597
817.194535	49309.864174	33.240615
817.813413	49377.828640	33.245632
818.485606	49469.734855	33.250650
819.639351	49541.647508	33.255668
820.130758	49627.824565	33.260685
821.193406	49712.121950	33.265703
821.715763	49783.448171	33.270720
822.673764	49862.464804	33.275738
823.465709	49950.381625	33.280756
823.949731	50035.454234	33.285773
825.097712	50126.035357	33.290791
825.776353	50221.787932	33.295808
826.452735	50293.864806	33.300826
827.463061	50377.438414	33.305844
828.187133	50477.069706	33.310861
829.303609	50551.378045	33.315879
830.078622	50621.894276	33.320896
830.956386	50728.943587	33.325914
832.048881	50784.180584	33.330932
832.754877	50884.135750	33.335949
833.889948	50962.368555	33.340967
834.111845	51028.206112	33.345984
834.783719	51128.130204	33.351002
836.168035	51190.999982	33.356020
836.726846	51262.641893	33.361037
837.460650	51329.131229	33.366055
838.148214	51402.848657	33.371072
839.010607	51482.758689	33.376090
839.742252	51571.024451	33.381108
840.259359	51656.591821	33.386125
841.619876	51723.576183	33.391143
842.157880	51813.227819	33.396160
842.546004	51904.478547	33.401178
843.828382	51990.083512	33.406196
844.338743	52067.416989	33.411213
845.432581	52170.088506	33.416231
846.316474	52244.611318	33.421248
846.855748	52339.766209	33.426266
847.643456	52441.743187	33.431284
848.617658	52531.029165	33.436301
849.694499	52623.777187	33.441319
850.259110	52701.515037	33.446336
851.069412	52800.100866	33.451354
852.438314	52891.531899	33.456372
853.385606	52990.841804	33.461389
854.267815	53072.933453	33.466407
855.303117	53164.614640	33.471424
856.002160	53271.622335	33.476442
856.954145	53336.752487	33.481460
857.783356	53432.637102	33.486477
858.664631	53517.426284	33.491495
859.511238	53600.526505	33.496512
860.389953	53711.396639	33.501530
861.553867	53784.524084	33.506548
862.144064	53874.111377	33.511565
863.229078	53957.124797	33.516583
863.885158	54039.332570	33.521600
864.482780	54132.477074	33.526618
865.637029	54221.540755	33.531636
866.531054	54325.304221	33.536653
867.502720	54400.178627	33.541671
868.485335	54488.052587	33.546688
869.228788	54585.819195	33.551706
870.200446	54669.365245	33.556724
871.078123	54754.814158	33.561741
872.054757	54834.540942	33.566759
872.306877	54929.887712	33.571776
873.256533	55024.622106	33.576794
874.169677	55106.901120	33.581812
875.054834	55203.247029	33.586829
875.642668	55308.845078	33.591847
876.718182	55379.319473	33.596864
877.586348	55500.205150	33.601882
878.983197	55566.999137	33.606900
879.634819	55663.491962	33.611917
880.563338	55763.224062	33.616935
881.827704	55824.958006	33.621952
882.407519	55907.012737	33.626970
883.292181	55986.945435	33.631988
883.691493	56060.232119	33.637005
884.814695	56151.005285	33.642023
886.243467	56204.068333	33.647040
886.312365	56302.200852	33.652058
887.374560	56385.601464	33.657076
887.746313	56487.724168	33.662093
889.055229	56563.425042	33.667111
889.571567	56647.412465	33.672128
890.167159	56756.777285	33.677146
891.539602	56833.031063	33.682164
891.930847	56946.937372	33.687181
893.053940	57028.130947	33.692199
893.860008	57132.344206	33.697216
894.670429	57233.053292	33.702234
895.745836	57334.762520	33.707252
897.118690	57425.281287	33.712269
898.052541	57513.442725	33.717287
898.923494	57613.086707	33.722304
899.874711	57717.488535	33.727322
901.106716	57779.859286	33.732340
901.831670	57890.558256	33.737357
902.353844	57999.692739	33.742375
903.712162	58070.432394	33.747392
904.328139	58179.843454	33.752410
905.151571	58266.494925	33.757428
906.219884	58357.521338	33.762445
906.814767	58461.311625	33.767463
907.817182	58551.727544	33.772480
909.159996	58649.748771	33.777498
909.986000	58737.484909	33.782516
910.806527	58837.228756	33.787533
911.846427	58936.859305	33.792551
912.881304	59026.852483	33.797568
913.806007	59130.294108	33.802586
914.741278	59220.199887	33.807604
915.821002	59312.558341	33.812621
916.580591	59396.194365	33.817639
917.912852	59486.925439	33.822656
918.475981	59585.287203	33.827674
919.144261	59663.656930	33.832692
920.198574	59765.600726	33.837709
920.954314	59866.209704	33.842727
922.269781	59948.550530	33.847744
922.590332	60055.686415	33.852762
923.886728	60137.358607	33.857780
924.794011	60242.046850	33.862797
925.627192	60336.953378	33.867815
926.740299	60443.611761	33.872832
927.399901	60533.968730	33.877850
928.576810	60613.650768	33.882868
929.468647	60718.985092	33.887885
930.327141	60826.759692	33.892903
931.463216	60875.257125	33.897920
932.237961	60986.020273	33.902938
933.190578	61060.343811	33.907956
933.804834	61147.326149	33.912973
934.425034	61244.418256	33.917991
935.270557	61320.111273	33.923008
935.966166	61431.821111	33.928026
937.457661	61519.603388	33.933044
938.148488	61612.682394	33.938061
938.711920	61708.886028	33.943079
940.153103	61792.793768	33.948096
940.783898	61909.647845	33.953114
941.597974	62012.090483	33.958132
942.592415	62113.794511	33.963149
943.550134	62206.407707	33.968167
944.523361	62311.299100	33.973184
944.828685	62436.061370	33.978202
945.892645	62519.416617	33.983220
947.006288	62644.048498	33.988237
948.298018	62748.597978	33.993255
949.156234	62848.985599	33.998272
950.037448	62969.418882	34.003290
951.272349	63075.643367	34.008308
952.056164	63195.064137	34.013325
952.857284	63308.006165	34.018343
954.429700	63415.321999	34.023360
955.007053	63528.171468	34.028378
956.177261	63620.262000	34.033396
957.573596	63731.731854	34.038413
958.405241	63827.464648	34.043431
959.333960	63924.126707	34.048448
960.505286	64044.185918	34.053466
961.527523	64131.764476	34.058484
962.245623	64221.971907	34.063501
963.356824	64344.985835	34.068519
964.529841	64423.689831	34.073536
965.091114	64543.713455	34.078554
966.442526	64646.934369	34.083572
967.266768	64732.393390	34.088589
967.529807	64881.858866	34.093607
968.627642	64957.977910	34.098624
970.055563	65083.482183	34.103642
970.817909	65172.717523	34.108660
971.759254	65305.902344	34.113677
972.862944	65406.510752	34.118695
974.098875	65502.895076	34.123712
974.663066	65642.622884	34.128730
975.836814	65719.768786	34.133748
976.671454	65829.044224	34.138765
977.543827	65951.468520	34.143783
979.090317	66038.107051	34.148800
979.789810	66152.967594	34.153818
980.671012	66258.350183	34.158836
982.136881	66361.729536	34.163853
982.773213	66461.912497	34.168871
984.001256	66552.514070	34.173888
984.932455	66649.420075	34.178906
985.516543	66734.414569	34.183924
986.669390	66834.751022	34.188941
987.231933	66943.766556	34.193959
988.616076	67007.021755	34.198976
989.209931	67134.608265	34.203994
990.221056	67206.700866	34.209012
990.878655	67340.112319	34.214029
991.927320	67420.114971	34.219047
992.762686	67545.735916	34.224064
994.126315	67682.726592	34.229082
994.926801	67759.441003	34.234100
995.860458	67881.744621	34.239117
996.732404	67986.528511	34.244135
997.625693	68124.986927	34.249152
998.617358	68200.762985	34.254170
999.465082	68341.043255	34.259188
1000.425308	68457.073151	34.264205
1001.657846	68576.914047	34.269223
1002.612967	68705.025147	34.274240
1003.870928	68813.523617	34.279258
1004.581117	68965.460783	34.284276
1006.321408	69044.602012	34.289293
1007.101745	69168.624909	34.294311
1008.285116	69273.612583	34.299328
1009.216879	69389.077656	34.304346
1010.525866	69514.756020	34.309364
1011.341912	69595.821797	34.314381
1012.347714	69741.652940	34.319399
1013.653839	69837.172697	34.324416
1014.163477	69950.667578	34.329434
1015.313780	70059.594449	34.334452
1016.712059	70210.490469	34.339469
1017.228609	70298.727128	34.344487
1019.022549	70415.924916	34.349504
1020.073343	70529.469743	34.354522
1021.071518	70617.871311	34.359540
1022.344157	70766.119045	34.364557
1023.233153	70845.365086	34.369575
1024.082425	70964.447595	34.374592
1025.223945	71063.379745	34.379610
1026.338063	71164.357547	34.384628
1027.411637	71290.994576	34.389645
1028.137161	71371.797769	34.394663
1029.052618	71523.311410	34.399680
1030.258500	71601.922483	34.404698
1030.880359	71738.010733	34.409716
1032.175434	71819.723477	34.414733
1032.980189	71964.396260	34.419751
1034.080983	72066.543406	34.424768
1035.031298	72177.655802	34.429786
1036.078899	72298.104896	34.434804
1037.418782	72398.395964	34.439821
1037.983226	72526.511997	34.444839
1039.231938	72623.665683	34.449856
1040.133600	72717.848367	34.454874
1041.150782	72836.940723	34.459892
1042.197170	72932.775886	34.464909
1042.798447	73059.423530	34.469927
1043.914938	73147.179396	34.474944
1044.981053	73270.550772	34.479962
1046.010924	73374.801183	34.484980
1047.083448	73509.471319	34.489997
1048.067499	73591.841150	34.495015
1048.833259	73736.526720	34.500032
1049.812928	73841.602719	34.505050
1050.986462	73973.239387	34.510068
1052.059556	74067.003080	34.515085
1052.933421	74227.517192	34.520103
1054.291754	74316.181305	34.525120
1055.004657	74468.811247	34.530138
1056.067451	74566.509528	34.535156
1057.500923	74717.882957	34.540173
1058.530777	74832.814417	34.545191
1059.246768	74967.848095	34.550208
1060.638495	75085.017406	34.555226
1061.554136	75223.686355	34.560244
1063.014752	75315.517353	34.565261
1063.777098	75479.724567	34.570279
1064.873083	75605.633432	34.575296
1065.954216	75700.364073	34.580314
1066.897041	75864.564674	34.585332
1068.269760	75965.614166	34.590349
1069.444025	76109.999074	34.595367
1070.129905	76223.482748	34.600384
1071.488256	76366.108568	34.605402
1072.262736	76502.141761	34.610420
1073.610240	76613.095533	34.615437
1074.189564	76792.396706	34.620455
1075.030407	76895.804334	34.625472
1077.223855	77003.996558	34.630490
1078.090082	77183.167071	34.635508
1079.379453	77271.810931	34.640525
1080.517340	77418.397733	34.645543
1081.720421	77536.590907	34.650560
1082.449953	77674.168605	34.655578
1083.516946	77768.342346	34.660596
1084.552743	77925.845296	34.665613
1085.365669	78037.713525	34.670631
1086.741562	78192.294974	34.675648
1087.922985	78309.446879	34.680666
1088.856010	78441.239408	34.685684
1090.048664	78589.557747	34.690701
1091.323285	78687.160070	34.695719
1091.997757	78832.326425	34.700736
1093.331366	78981.952528	34.705754
1094.320221	79081.074903	34.710772
1095.351966	79243.013156	34.715789
1096.275099	79349.757512	34.720807
1097.500216	79487.894347	34.725824
1098.622671	79614.917326	34.730842
1099.594648	79705.107644	34.735860
1100.566006	79865.391677	34.740877
1102.085003	79955.287503	34.745895
1102.657299	80099.170604	34.750912
1103.812436	80208.233947	34.755930
1104.744953	80332.345933	34.760948
1105.992419	80475.650197	34.765965
1107.123323	80588.139153	34.770983
1108.081827	80721.073739	34.776000
1109.520658	80859.723084	34.781018
1110.161826	80989.454399	34.786036
1111.346695	81133.841481	34.791053
1112.533662	81250.990295	34.796071
1113.855168	81374.231205	34.801088
1115.001089	81526.440516	34.806106
1115.946246	81642.650165	34.811124
1117.395029	81780.564468	34.816141
1118.369876	81934.555045	34.821159
1119.663680	82059.732519	34.826176
1120.744552	82189.565760	34.831194
1121.957166	82326.655168	34.836212
1123.199465	82491.645068	34.841229
1124.187513	82584.955685	34.846247
1125.510293	82726.221556	34.851264
1126.692358	82880.647655	34.856282
1127.695486	82979.558836	34.861300
1129.028275	83121.154524	34.866317
1130.071931	83246.372570	34.871335
1130.992018	83400.749334	34.876352
1132.511673	83536.533435	34.881370
1133.874258	83637.388341	34.886388
1134.774814	83787.440400	34.891405
1135.615250	83900.764736	34.896423
1137.295097	84051.434452	34.901440
1138.362242	84167.727242	34.906458
1138.991306	84324.692303	34.911476
1140.656174	84443.167602	34.916493
1141.978981	84546.378792	34.921511
1142.579080	84722.558864	34.926528
1143.916918	84822.791142	34.931546
1144.947817	84997.798567	34.936564
1146.244760	85089.010039	34.941581
1147.522784	85265.725407	34.946599
1148.397547	85374.733853	34.951616
1149.997093	85508.380896	34.956634
1150.939340	85642.392535	34.961652
1152.135027	85796.332013	34.966669
1153.585268	85903.051339	34.971687
1154.360330	86041.518040	34.976704
1155.761090	86177.546680	34.981722
1156.895823	86287.416319	34.986740
1157.998552	86449.500250	34.991757
1159.128358	86544.633179	34.996775
1159.904807	86698.348660	35.001792
1161.530387	86794.017203	35.006810
1161.901925	86925.693284	35.011828
1163.592122	87022.939677	35.016845
1164.543900	87176.030015	35.021863
1165.772957	87271.586701	35.026880
1166.951741	87425.420480	35.031898
1167.747940	87518.410300	35.036916
1168.994397	87682.776070	35.041933
1170.335072	87791.501466	35.046951
1171.661523	87895.240520	35.051968
1172.624973	88069.044480	35.056986
1173.436380	88195.877888	35.062004
1174.266272	88303.978865	35.067021
1176.305893	88426.147618	35.072039
1176.986470	88587.549683	35.077056
1178.815623	88724.753160	35.082074
1179.734608	88841.853844	35.087092
1181.173704	88991.901172	35.092109
1182.485519	89107.492705	35.097127
1183.285922	89227.011029	35.102144
1184.597763	89383.986878	35.107162
1185.722797	89503.404518	35.112180
1186.919314	89654.766108	35.117197
1188.405737	89761.037233	35.122215
1188.954894	89927.687425	35.127232
1190.578455	90031.319940	35.132250
1191.370832	90218.682781	35.137268
1192.664319	90328.851366	35.142285
1194.328861	90492.172808	35.147303
1195.180930	90611.994093	35.152320
1196.722586	90766.944947	35.157338
1197.872223	90882.002530	35.162356
1199.106794	91042.000327	35.167373
1200.253880	91159.722311	35.172391
1201.358133	91324.441876	35.177408
1203.018626	91448.977369	35.182426
1204.087609	91581.911633	35.187444
1205.094659	91715.400456	35.192461
1206.492550	91878.293986	35.197479
1207.509821	91991.386212	35.202496
1209.081314	92162.539448	35.207514
1209.987503	92272.197533	35.212532
1211.358387	92427.901969	35.217549
1212.636032	92539.532557	35.222567
1213.765320	92702.335749	35.227584
1215.016007	92808.507375	35.232602
1216.202515	92987.223127	35.237620
1217.428015	93088.340214	35.242637
1218.947467	93260.680351	35.247655
1219.855498	93394.233032	35.252672
1221.344056	93503.437794	35.257690
1222.741449	93664.902492	35.262708
1223.742809	93760.289834	35.267725
1225.350494	93907.826664	35.272743
1225.889196	94057.235896	35.277760
1227.093147	94141.713381	35.282778
1228.935358	94238.019076	35.287796
1229.584983	94405.401940	35.292813
1230.783870	94514.910743	35.297831
1232.065496	94626.380433	35.302848
1233.646865	94775.021480	35.307866
1234.187563	94892.423310	35.312884
1235.123944	95023.988764	35.317901
1237.202668	95139.110581	35.322919
1238.051793	95271.279631	35.327936
1239.215953	95405.100949	35.332954
1240.217042	95572.177323	35.337972
1241.439429	95687.646850	35.342989
1243.001105	95805.745112	35.348007
1243.914618	95994.314181	35.353024
1245.168117	96096.692966	35.358042
1246.479656	96248.979715	35.363060
1247.212166	96412.695434	35.368077
1249.056217	96530.771593	35.373095
1250.170388	96688.577215	35.378112
1251.620884	96843.028326	35.383130
1252.601082	96973.314055	35.388148
1254.312880	97100.283262	35.393165
1255.415380	97265.958021	35.398183
1256.888440	97370.863420	35.403200
1258.268242	97542.303477	35.408218
1259.742792	97645.622051	35.413236
1260.854439	97806.168775	35.418253
1262.548959	97964.435086	35.423271
1263.471117	98077.712417	35.428288
1265.255206	98188.101340	35.433306
1266.737594	98322.939536	35.438324
1267.548129	98491.649365	35.443341
1268.769516	98630.067333	35.448359
1270.003347	98734.814618	35.453376
1271.347368	98909.389618	35.458394
1272.397585	99036.449514	35.463412
1273.484864	99148.788564	35.468429
1275.085721	99329.924582	35.473447
1276.337262	99466.046247	35.478464
1277.731535	99583.754269	35.483482
1278.835426	99751.363861	35.488500
1280.230837	99869.864016	35.493517
1281.762540	100033.504030	35.498535
1282.894873	100143.240460	35.503552
1284.600633	100279.376991	35.508570
1285.844925	100432.195910	35.513588
1287.189347	100548.936125	35.518605
1288.484963	100708.733702	35.523623
1289.711920	100828.524647	35.528640
1290.951609	100971.085385	35.533658
1292.125486	101080.452700	35.538676
1292.961954	101259.605819	35.543693
1294.563583	101373.190018	35.548711
1295.779675	101508.918114	35.553728
1296.607252	101644.082360	35.558746
1297.757892	101747.312732	35.563764
1298.834470	101866.936804	35.568781
1300.182264	102039.997367	35.573799
1301.390866	102201.381925	35.578816
1302.872394	102337.572533	35.583834
1303.680551	102469.467031	35.588852
1304.872735	102606.932739	35.593869
1306.553724	102714.284584	35.598887
1307.674036	102884.014975	35.603904
1309.035699	103052.290839	35.608922
1309.944912	103184.489689	35.613940
1310.883064	103343.963539	35.618957
1313.058720	103472.444492	35.623975
1314.559650	103664.172324	35.628992
1315.644724	103826.188863	35.634010
1316.572493	103963.742525	35.639028
1317.348861	104109.933381	35.644045
1319.387752	104255.335968	35.649063
1320.826878	104406.631251	35.654080
1322.104303	104605.059344	35.659098
1323.267100	104747.750256	35.664116
1324.305671	104914.793526	35.669133
1326.472605	105052.517276	35.674151
1327.723931	105244.816533	35.679168
1328.889518	105387.074204	35.684186
1330.623743	105513.832891	35.689204
1332.144062	105669.717699	35.694221
1333.728448	105822.568372	35.699239
1334.937006	105978.352872	35.704256
1336.529471	106126.438897	35.709274
1337.828030	106273.313181	35.714292
1338.793625	106456.491290	35.719309
1340.058347	106628.693743	35.724327
1341.722888	106754.887881	35.729344
1342.768886	106931.956037	35.734362
1344.428842	107065.772290	35.739380
1345.628781	107241.584162	35.744397
1347.415404	107366.009048	35.749415
1348.299684	107540.145511	35.754432
1349.951724	107665.036356	35.759450
1351.546766	107848.485797	35.764468
1352.805392	108009.098188	35.769485
1353.658474	108137.162700	35.774503
1355.741454	108266.158992	35.779520
1356.794199	108408.452546	35.784538
1358.117685	108620.577456	35.789556
1359.452957	108779.606832	35.794573
1360.584671	108892.618259	35.799591
1361.988205	109028.062137	35.804608
1363.015826	109200.466223	35.809626
1364.956266	109362.555227	35.814644
1365.726946	109514.767522	35.819661
1367.552839	109699.529793	35.824679
1368.937922	109844.494265	35.829696
1369.737363	109976.678492	35.834714
1370.846285	110108.902864	35.839732
1372.772502	110240.143573	35.844749
1373.918748	110428.456324	35.849767
1375.085194	110554.008889	35.854784
1376.175034	110697.278361	35.859802
1378.037830	110832.551672	35.864820
1379.606525	110972.961584	35.869837
1380.450073	111125.666040	35.874855
1381.948559	111272.887012	35.879872
1383.170256	111429.305830	35.884890
1384.725707	111578.127360	35.889908
1386.297733	111761.261771	35.894925
1387.225508	111928.731915	35.899943
1388.663418	112102.895259	35.904960
1390.284539	112282.879706	35.909978
1391.690622	112432.926509	35.914996
1392.933733	112610.264117	35.920013
1394.356143	112762.228357	35.925031
1395.880108	112918.133790	35.930048
1397.236224	113092.627265	35.935066
1398.330118	113235.011908	35.940084
1399.798336	113393.777825	35.945101
1401.617657	113537.295999	35.950119
1402.915005	113709.967320	35.955136
1404.557440	113888.269772	35.960154
1406.167521	114035.179217	35.965172
1407.127666	114234.293380	35.970189
1408.682874	114429.123688	35.975207
1410.236779	114576.450394	35.980224
1411.841252	114756.107153	35.985242
1413.251673	114929.047452	35.990260
1414.548185	115082.755108	35.995277
1416.110769	115220.758961	36.000295
1417.929012	115404.647023	36.005312
1419.161466	115557.703011	36.010330
1420.774118	115743.094976	36.015348
1421.970083	115871.024788	36.020365
1423.326317	116078.593087	36.025383
1424.673586	116224.259204	36.030400
1426.561644	116391.068441	36.035418
1427.948931	116554.140662	36.040436
1429.491698	116700.766107	36.045453
1430.469951	116900.594821	36.050471
1432.299162	117026.720397	36.055488
1433.227364	117218.860730	36.060506
1435.413906	117347.090092	36.065524
1436.673434	117526.865618	36.070541
1438.084240	117683.571938	36.075559
1439.760425	117859.744324	36.080576
1441.184765	117990.428009	36.085594
1442.658885	118160.227079	36.090612
1444.109853	118307.566465	36.095629
1445.479986	118478.365556	36.100647
1446.777928	118607.527545	36.105664
1448.106204	118736.558730	36.110682
1449.479632	118905.530268	36.115700
1450.781345	119014.805729	36.120717
1452.139172	119209.317738	36.125735
1453.748144	119333.476136	36.130752
1454.593637	119489.004234	36.135770
1456.236661	119625.999674	36.140788
1457.904391	119768.310747	36.145805
1458.937082	119967.743041	36.150823
1460.624571	120118.556762	36.155840
1461.961033	120284.320157	36.160858
1463.546666	120424.843229	36.165876
1464.675499	120600.025801	36.170893
1466.530078	120729.958431	36.175911
1468.011312	120922.880604	36.180928
1469.351000	121114.218292	36.185946
1470.839677	121266.817945	36.190964
1471.864684	121413.058494	36.195981
1473.641440	121556.432166	36.200999
1475.273664	121770.233437	36.206016
1476.382034	121941.299478	36.211034
1477.548631	122096.602094	36.216052
1479.715533	122250.809480	36.221069
1480.901311	122456.353621	36.226087
1482.576662	122647.687120	36.231104
1484.092853	122822.620311	36.236122
1485.871774	122982.795672	36.241140
1487.018056	123155.396061	36.246157
1488.376901	123323.606833	36.251175
1490.800191	123476.032777	36.256192
1492.180274	123643.710243	36.261210
1493.414497	123859.022841	36.266228
1495.027077	124038.597089	36.271245
1496.337238	124197.726971	36.276263
1498.290731	124345.090127	36.281280
1499.780754	124551.919389	36.286298
1501.067264	124717.857861	36.291316
1502.387369	124869.453730	36.296333
1503.852564	125076.822967	36.301351
1505.411448	125219.060384	36.306368
1507.013522	125402.407385	36.311386
1508.266273	125588.648463	36.316404
1510.116858	125741.102298	36.321421
1511.568947	125953.610390	36.326439
1513.098192	126106.839349	36.331456
1514.995885	126283.406569	36.336474
1516.334692	126470.070720	36.341492
1518.273923	126612.888406	36.346509
1519.727314	126778.977704	36.351527
1521.405346	126986.264427	36.356544
1522.412968	127171.275913	36.361562
1523.909736	127313.838217	36.366580
1525.922506	127463.717138	36.371597
1527.082192	127664.288885	36.376615
1528.556234	127808.542177	36.381632
1530.014281	127934.937223	36.386650
1531.663310	128120.106585	36.391668
1532.632185	128266.089353	36.396685
1534.420565	128403.087797	36.401703
1536.063358	128547.001465	36.406720
1537.054794	128768.497608	36.411738
1538.653856	128911.203984	36.416756
1540.058563	129067.801066	36.421773
1541.810930	129229.791201	36.426791
1543.159420	129404.096814	36.431808
1544.225147	129591.801057	36.436826
1545.954492	129763.983464	36.441844
1547.717721	129939.379400	36.446861
1549.423660	130096.301835	36.451879
1550.676489	130262.038618	36.456896
1552.275204	130474.305022	36.461914
1553.828541	130685.351353	36.466932
1555.424439	130862.299960	36.471949
1557.077000	131033.349520	36.476967
1558.526133	131205.978086	36.481984
1560.272007	131365.194441	36.487002
1561.872574	131557.501918	36.492020
1563.475428	131771.158454	36.497037
1564.980886	131958.935429	36.502055
1566.745955	132110.893283	36.507072
1568.062333	132340.474719	36.512090
1569.562813	132502.422471	36.517108
1571.144021	132678.396583	36.522125
1573.239981	132846.523323	36.527143
1574.642447	133078.998493	36.532160
1576.021353	133276.560276	36.537178
1577.757080	133426.743355	36.542196
1579.253076	133634.703965	36.547213
1580.819202	133826.905614	36.552231
1582.807293	134011.236500	36.557248
1584.363166	134233.915086	36.562266
1585.694985	134395.165495	36.567284
1587.613985	134552.306921	36.572301
1588.872396	134792.611409	36.577319
1590.861746	134953.545110	36.582336
1592.745680	135129.232817	36.587354
1594.365900	135343.851025	36.592372
1595.735882	135507.559794	36.597389
1597.712058	135674.366359	36.602407
1599.280524	135888.173194	36.607424
1600.824120	136070.902582	36.612442
1602.653213	136215.877459	36.617460
1604.206655	136451.308359	36.622477
1605.784361	136610.339891	36.627495
1607.577719	136760.607234	36.632512
1608.973299	136967.568724	36.637530
1610.551883	137140.858781	36.642548
1612.356732	137324.023388	36.647565
1613.676711	137482.606396	36.652583
1615.376669	137672.290584	36.657600
1616.560338	137811.217253	36.662618
1618.241869	137991.072833	36.667636
1619.543222	138164.336928	36.672653
1621.102854	138313.242725	36.677671
1622.600666	138504.396357	36.682688
1623.940265	138686.109968	36.687706
1625.402364	138855.804278	36.692724
1627.246566	139036.083926	36.697741
1628.572308	139235.772974	36.702759
1629.973009	139413.033191	36.707776
1631.847474	139600.877148	36.712794
1633.054661	139814.136260	36.717812
1634.907258	139973.813944	36.722829
1636.743254	140193.401150	36.727847
1638.368876	140396.396057	36.732864
1639.712386	140576.789883	36.737882
1641.511248	140804.397009	36.742900
1643.178161	141000.723219	36.747917
1644.854952	141180.877636	36.752935
1646.423850	141419.146397	36.757952
1647.715178	141604.345316	36.762970
1650.131882	141784.449197	36.767988
1652.083854	141976.224590	36.773005
1653.223314	142212.438571	36.778023
1654.985079	142445.716555	36.783040
1656.264208	142656.360790	36.788058
1658.157264	142858.810111	36.793076
1659.883792	143038.942311	36.798093
1661.703691	143227.070990	36.803111
1663.618345	143476.289689	36.808128
1665.255064	143704.565342	36.813146
1666.914813	143904.181478	36.818164
1668.586003	144111.300575	36.823181
1670.288888	144304.537030	36.828199
1672.351583	144496.462734	36.833216
1673.619378	144701.621855	36.838234
1675.723798	144889.943662	36.843252
1677.432212	145120.842145	36.848269
1678.931881	145307.145756	36.853287
1681.022676	145540.432964	36.858304
1682.596955	145717.322045	36.863322
1684.521384	145934.249253	36.868340
1686.135299	146141.695199	36.873357
1687.817038	146315.249583	36.878375
1689.359176	146545.310377	36.883392
1691.082620	146728.303889	36.888410
1693.062172	146915.871841	36.893428
1694.815902	147156.627352	36.898445
1696.329882	147325.916773	36.903463
1698.401769	147539.307683	36.908480
1700.076945	147729.882354	36.913498
1701.865198	147917.245777	36.918516
1703.582228	148135.653498	36.923533
1705.054035	148295.815090	36.928551
1706.853541	148497.872204	36.933568
1708.142317	148686.067380	36.938586
1709.645298	148858.624610	36.943604
1711.449118	148994.701947	36.948621
1712.843647	149221.230726	36.953639
1714.098362	149398.482690	36.958656
1715.856812	149562.458895	36.963674
1717.451728	149797.466178	36.968692
1719.467945	149971.063475	36.973709
1721.095370	150160.608002	36.978727
1722.471289	150405.580750	36.983744
1723.988162	150588.375645	36.988762
1726.004811	150787.534892	36.993780
1727.981639	151004.893971	36.998797
1729.193713	151207.910742	37.003815
1731.254481	151383.777826	37.008832
1733.166054	151640.579184	37.013850
1734.548767	151840.111747	37.018868
1736.986627	152024.834958	37.023885
1738.348104	152273.361166	37.028903
1740.208850	152449.760176	37.033920
1742.011638	152703.468299	37.038938
1743.417718	152872.093945	37.043956
1745.665675	153124.555542	37.048973
1746.950786	153327.003269	37.053991
1749.045764	153537.108266	37.059008
1751.034013	153762.547300	37.064026
1752.404128	153961.004306	37.069044
1754.774202	154173.884315	37.074061
1756.000147	154405.318992	37.079079
1758.123612	154582.422999	37.084096
1759.917352	154850.869163	37.089114
1761.599094	155055.736804	37.094132
1763.202299	155264.219049	37.099149
1764.907059	155485.162853	37.104167
1766.590577	155706.682044	37.109184
1769.439905	155887.608278	37.114202
1771.088989	156102.440795	37.119220
1772.992766	156320.505566	37.124237
1774.354881	156571.802371	37.129255
1776.243417	156791.939365	37.134272
1778.411752	156990.946802	37.139290
1780.150297	157173.438325	37.144308
1782.082483	157416.320143	37.149325
1783.841270	157597.390551	37.154343
1785.468664	157800.698342	37.159360
1787.711107	158032.275307	37.164378
1788.999800	158231.226692	37.169396
1791.198673	158412.231516	37.174413
1792.569160	158649.923486	37.179431
1794.633312	158848.945520	37.184448
1796.579626	159042.839086	37.189466
1798.094192	159259.703529	37.194484
1799.801534	159479.962515	37.199501
1801.886773	159656.528239	37.204519
1803.003909	159856.188228	37.209536
1805.139480	160055.269208	37.214554
1806.730280	160238.104653	37.219572
1808.853273	160420.336642	37.224589
1810.207261	160613.813011	37.229607
1811.845886	160814.296011	37.234624
1813.735553	161019.318242	37.239642
1815.118890	161195.724123	37.244660
1817.425908	161421.530578	37.249677
1819.076814	161602.930537	37.254695
1820.462641	161821.593902	37.259712
1822.419466	162036.185926	37.264730
1824.082472	162231.638433	37.269748
1825.891556	162457.847532	37.274765
1827.620833	162682.092353	37.279783
1829.219676	162868.085148	37.284800
1831.306958	163115.559898	37.289818
1833.191270	163334.736723	37.294836
1834.946136	163551.411669	37.299853
1836.715550	163776.506622	37.304871
1839.037407	164012.726470	37.309888
1841.128029	164205.103388	37.314906
1842.841975	164459.736037	37.319924
1844.956557	164649.435490	37.324941
1846.450642	164890.802029	37.329959
1848.652734	165093.299368	37.334976
1850.405037	165327.855222	37.339994
1852.095983	165536.815584	37.345012
1853.972217	165783.619004	37.350029
1856.038166	165974.639359	37.355047
1857.767915	166234.215471	37.360064
1859.842338	166431.121796	37.365082
1861.867968	166672.199986	37.370100
1863.957447	166870.615555	37.375117
1865.747470	167132.192322	37.380135
1867.237687	167327.648730	37.385152
1870.279794	167505.597538	37.390170
1871.796413	167777.889060	37.395188
1873.471544	167964.681880	37.400205
1876.019322	168184.454422	37.405223
1877.973307	168400.339763	37.410240
1879.365123	168629.595618	37.415258
1881.080002	168817.185424	37.420276
1883.196752	169055.511990	37.425293
1885.303202	169260.431680	37.430311
1886.629386	169474.976770	37.435328
1889.313146	169678.564025	37.440346
1890.912946	169900.970372	37.445364
1892.830312	170136.050070	37.450381
1894.582709	170322.360175	37.455399
1896.351221	170566.903376	37.460416
1898.547233	170762.557141	37.465434
1900.037768	170989.819943	37.470452
1902.205828	171207.424916	37.475469
1903.604599	171402.345871	37.480487
1905.254739	171604.673938	37.485504
1907.126330	171805.090533	37.490522
1909.040405	172034.981419	37.495540
1910.632500	172212.306962	37.500557
1912.802480	172432.252507	37.505575
1914.545512	172617.649058	37.510592
1916.559852	172860.429727	37.515610
1917.982934	173058.526368	37.520628
1920.292101	173244.838159	37.525645
1922.064738	173451.393207	37.530663
1923.811704	173714.277294	37.535680
1925.926941	173905.062907	37.540698
1927.777650	174140.075698	37.545716
1929.586224	174341.428512	37.550733
1931.670365	174576.990366	37.555751
1933.429895	174787.499692	37.560768
1935.435336	175034.912669	37.565786
1937.296769	175255.138416	37.570804
1939.308239	175475.493785	37.575821
1941.598346	175718.615914	37.580839
1943.101634	175975.831950	37.585856
1945.598031	176166.237931	37.590874
1947.275745	176448.814637	37.595892
1949.311019	176643.292239	37.600909
1951.343156	176895.393595	37.605927
1953.523694	177107.256311	37.610944
1955.353633	177362.564267	37.615962
1957.332327	177567.775482	37.620980
1959.139239	177840.039562	37.625997
1960.765308	178053.872762	37.631015
1963.485878	178259.388339	37.636032
1965.215715	178537.949265	37.641050
1967.071357	178767.633898	37.646068
1969.517048	178972.194314	37.651085
1971.724353	179232.236905	37.656103
1973.583892	179459.273056	37.661120
1975.669244	179689.776320	37.666138
1977.662400	179920.181281	37.671156
1979.786808	180167.441107	37.676173
1981.742531	180365.158607	37.681191
1983.593428	180636.596397	37.686208
1985.783195	180830.358418	37.691226
1987.791504	181075.967140	37.696244
1989.309054	181309.969586	37.701261
1992.129987	181530.938967	37.706279
1993.957652	181784.358106	37.711296
1996.279617	181970.795979	37.716314
1998.190066	182233.771425	37.721332
2000.223413	182444.859478	37.726349
2002.590265	182640.542816	37.731367
2004.064773	182911.445560	37.736384
2006.555027	183091.847248	37.741402
2008.040931	183349.288484	37.746420
2010.091696	183541.067187	37.751437
2012.129083	183778.032949	37.756455
2013.949430	183953.469014	37.761472
2016.002774	184201.169111	37.766490
2017.550568	184384.910487	37.771508
2019.869616	184591.966531	37.776525
2021.596713	184783.269025	37.781543
2023.504759	184988.932895	37.786560
2025.564104	185213.480329	37.791578
2027.847415	185420.812345	37.796596
2029.318498	185643.285423	37.801613
2031.761344	185837.816091	37.806631
2033.677685	186088.974427	37.811648
2035.859251	186280.312687	37.816666
2037.498951	186508.613030	37.821684
2039.487013	186740.158500	37.826701
2041.610596	186940.530923	37.831719
2043.539484	187197.784328	37.836736
2045.964816	187392.527444	37.841754
2047.790575	187653.784298	37.846772
2049.979839	187871.141852	37.851789
2052.093845	188074.477440	37.856807
2054.092618	188333.680309	37.861824
2056.190942	188536.627020	37.866842
2058.384945	188800.509476	37.871860
2060.306998	189019.386822	37.876877
2062.927855	189254.829150	37.881895
2064.663364	189467.875341	37.886912
2066.995485	189729.203062	37.891930
2068.854780	189937.016037	37.896948
2071.380488	190163.264827	37.901965
2073.415653	190421.915043	37.906983
2075.298911	190627.772906	37.912000
2078.063538	190872.261470	37.917018
2079.998790	191081.552176	37.922036
2081.964241	191321.017415	37.927053
2084.242688	191522.336616	37.932071
2086.561013	191778.994848	37.937088
2088.323851	191982.237920	37.942106
2090.826197	192225.810444	37.947124
2092.942761	192426.930643	37.952141
2095.250018	192661.411489	37.957159
2097.293343	192885.274817	37.962176
2099.856283	193087.697559	37.967194
2101.855080	193306.975680	37.972212
2104.010785	193539.276485	37.977229
2106.210104	193733.548321	37.982247
2107.883897	193955.787175	37.987264
2110.344806	194181.849194	37.992282
2112.308942	194393.548149	37.997300
2114.317913	194605.177429	38.002317
2116.650094	194808.087992	38.007335
2118.829184	195050.761136	38.012352
2120.908644	195232.277336	38.017370
2122.677462	195482.569179	38.022388
2124.885284	195666.313012	38.027405
2127.354735	195901.709861	38.032423
2129.296788	196073.224311	38.037440
2131.375456	196265.532433	38.042458
2133.437680	196464.761015	38.047476
2134.836272	196645.920647	38.052493
2137.472265	196814.712954	38.057511
2139.000878	197052.206201	38.062528
2141.423399	197211.641494	38.067546
2143.433440	197449.732888	38.072564
2145.256820	197638.380491	38.077581
2147.387840	197856.933852	38.082599
2149.424207	198057.149970	38.087616
2151.594129	198277.234693	38.092634
2153.828587	198509.126799	38.097652
2155.606199	198701.999391	38.102669
2157.671148	198953.086047	38.107687
2159.664588	199160.091003	38.112704
2162.031493	199403.135536	38.117722
2164.053503	199620.482295	38.122740
2165.864956	199853.170843	38.127757
2168.426392	200108.499743	38.132775
2170.639005	200332.863693	38.137792
2172.937779	200563.053675	38.142810
2175.337731	200807.444770	38.147828
2177.514329	201058.548948	38.152845
2179.628966	201265.403153	38.157863
2181.760667	201532.357654	38.162880
2183.831918	201749.032402	38.167898
2186.068603	202002.073438	38.172916
2188.441877	202235.596981	38.177933
2190.920325	202465.461821	38.182951
2193.126635	202734.834739	38.187968
2195.415302	202948.585588	38.192986
2198.326422	203174.284731	38.198004
2200.304609	203421.559561	38.203021
2203.157948	203637.851067	38.208039
2204.966494	203895.728703	38.213056
2207.107431	204090.200163	38.218074
2209.452416	204360.955179	38.223092
2211.817148	204571.970937	38.228109
2214.407749	204792.611731	38.233127
2216.606223	205029.030699	38.238144
2218.659563	205241.951623	38.243162
2220.689937	205490.966225	38.248180
2223.056989	205703.762935	38.253197
2225.459931	205912.060997	38.258215
2227.123281	206183.072289	38.263232
2229.848399	206378.461674	38.268250
2232.058085	206638.776026	38.273268
2233.809819	206850.735100	38.278285
2236.584137	207073.919671	38.283303
2238.229391	207302.831604	38.288320
2240.688478	207556.026925	38.293338
2243.122083	207765.697678	38.298356
2245.290057	207987.433084	38.303373
2247.728591	208232.116436	38.308391
2249.636929	208433.824395	38.313408
2252.178786	208623.601067	38.318426
2253.938931	208841.925917	38.323444
2255.550165	209062.941077	38.328461
2257.959480	209238.217792	38.333479
2260.003702	209475.935716	38.338496
2262.107828	209672.767267	38.343514
2264.367990	209917.879210	38.348532
2266.524363	210128.465324	38.353549
2269.025289	210343.390025	38.358567
2270.744933	210596.029677	38.363584
2272.895545	210822.361037	38.368602
2275.523920	211055.536368	38.373620
2277.596073	211304.936472	38.378637
2279.527946	211523.992547	38.383655
2281.855068	211804.546638	38.388672
2283.935425	212037.939430	38.393690
2286.065816	212282.789164	38.398708
2288.541080	212551.503543	38.403725
2290.915535	212792.990289	38.408743
2292.866883	213078.789320	38.413760
2295.344281	213326.406420	38.418778
2297.599966	213576.090930	38.423796
2299.920330	213843.095887	38.428813
2302.587261	214130.220675	38.433831
2305.458071	214368.333619	38.438848
2307.404428	214673.882482	38.443866
2310.498060	214912.254053	38.448884
2312.622839	215161.927202	38.453901
2314.699116	215437.166197	38.458919
2317.370026	215680.101926	38.463936
2319.327860	215956.707598	38.468954
2322.222593	216201.514135	38.473972
2324.264023	216460.625879	38.478989
2326.456712	216738.619456	38.484007
2329.279145	216977.930012	38.489024
2331.551510	217241.896179	38.494042
2334.167273	217517.197642	38.499060
2336.373053	217780.605058	38.504077
2339.062810	218028.700851	38.509095
2340.964501	218292.425014	38.514112
2343.658101	218557.903719	38.519130
2345.924963	218792.585373	38.524148
2348.315304	219069.591876	38.529165
2350.506692	219302.204893	38.534183
2352.987284	219594.676496	38.539200
2355.467137	219832.248043	38.544218
2357.639182	220104.328625	38.549236
2360.066865	220369.348261	38.554253
2362.502467	220611.220927	38.559271
2364.376434	220889.446229	38.564288
2366.803495	221173.057348	38.569306
2369.296034	221404.283387	38.574324
2371.224594	221745.189088	38.579341
2373.205536	222009.269589	38.584359
2375.785671	222263.809235	38.589376
2377.710213	222502.493100	38.594394
2380.002569	222751.835990	38.599412
2382.590961	223000.307428	38.604429
2384.568220	223265.878439	38.609447
2386.910830	223511.584337	38.614464
2389.107072	223777.757254	38.619482
2391.296282	224038.434132	38.624500
2393.507051	224315.132861	38.629517
2396.005086	224583.089114	38.634535
2398.214303	224868.500618	38.639552
2400.502693	225147.488216	38.644570
2402.758579	225427.777107	38.649588
2405.015566	225727.659576	38.654605
2407.513250	226022.057595	38.659623
2409.743650	226318.708478	38.664640
2412.400864	226615.343565	38.669658
2415.303292	226909.045693	38.674676
2417.603528	227209.218738	38.679693
2419.693275	227508.486554	38.684711
2422.617409	227803.229612	38.689728
2424.784417	228105.915792	38.694746
2427.297086	228408.141909	38.699764
2429.751024	228715.864059	38.704781
2432.253520	229020.557397	38.709799
2434.866665	229325.437434	38.714816
2437.143243	229633.317908	38.719834
2440.143829	229931.332271	38.724852
2442.556879	230242.139271	38.729869
2444.939615	230555.288686	38.734887
2447.578163	230852.017439	38.739904
2450.033939	231164.420862	38.744922
2452.927006	231459.892183	38.749940
2455.256657	231766.450846	38.754957
2457.893796	232062.523396	38.759975
2460.317794	232365.995976	38.764992
2462.994183	232670.750213	38.770010
2465.777799	232970.942233	38.775028
2468.003371	233267.134580	38.780045
2470.193148	233571.460853	38.785063
2473.261629	233871.966112	38.790080
2475.829663	234175.370796	38.795098
2478.357431	234465.626543	38.800116
2480.700860	234770.744933	38.805133
2483.467720	235057.611950	38.810151
2485.827472	235372.457146	38.815168
2488.226047	235668.476895	38.820186
2490.594873	235964.095839	38.825204
2493.361210	236252.083851	38.830221
2495.743505	236558.014205	38.835239
2498.496563	236841.332595	38.840256
2500.587308	237162.372385	38.845274
2503.170623	237448.462381	38.850292
2505.445648	237749.358804	38.855309
2508.075216	238040.395852	38.860327
2510.367289	238311.853647	38.865344
2512.324890	238585.955834	38.870362
2514.783415	238859.928527	38.875380
2517.142714	239140.165850	38.880397
2519.396271	239424.052741	38.885415
2521.915998	239703.478669	38.890432
2523.967078	240001.597377	38.895450
2526.514475	240288.538607	38.900468
2528.612999	240611.619146	38.905485
2531.507814	240915.270634	38.910503
2534.203618	241209.124736	38.915520
2536.356306	241532.097625	38.920538
2539.229617	241833.646690	38.925556
2541.579929	242157.529741	38.930573
2544.145735	242472.667300	38.935591
2546.726462	242785.872896	38.940608
2548.978637	243103.246165	38.945626
2551.670218	243425.910059	38.950644
2553.972612	243755.342116	38.955661
2556.523927	244094.692515	38.960679
2559.210552	244410.755589	38.965696
2561.505184	244762.772406	38.970714
2564.562794	245098.692329	38.975732
2567.423691	245438.124149	38.980749
2569.642946	245775.982041	38.985767
2572.633240	246104.320334	38.990784
2574.967796	246456.157431	38.995802
2577.851164	246779.383302	39.000820
2580.572635	247118.257122	39.005837
2583.102627	247459.524373	39.010855
2586.342290	247797.606466	39.015872
2588.557453	248145.300861	39.020890
2591.221984	248478.395420	39.025908
2593.728178	248804.225657	39.030925
2596.456168	249152.476164	39.035943
2599.329368	249488.105401	39.040960
2601.737137	249827.187480	39.045978
2604.835627	250160.089917	39.050996
2607.181985	250498.090893	39.056013
2609.800150	250847.708812	39.061031
2612.572793	251173.171500	39.066048
2615.182045	251515.857611	39.071066
2617.775875	251852.018627	39.076084
2620.420960	252186.165446	39.081101
2623.085907	252529.022569	39.086119
2625.639959	252874.488911	39.091136
2628.134197	253216.358329	39.096154
2631.255868	253549.466937	39.101172
2633.892384	253893.906074	39.106189
2636.473793	254223.240377	39.111207
2639.089940	254564.356298	39.116224
2641.648196	254909.571729	39.121242
2644.178983	255240.897145	39.126260
2646.842012	255595.546767	39.131277
2649.091577	255925.876365	39.136295
2651.548494	256230.060115	39.141312
2654.062609	256550.721337	39.146330
2656.871321	256863.614064	39.151348
2659.309585	257183.170539	39.156365
2661.589198	257513.294608	39.161383
2664.512816	257828.507520	39.166400
2666.406058	258173.198547	39.171418
2669.217883	258501.156728	39.176436
2671.902482	258835.181323	39.181453
2674.236619	259176.755653	39.186471
2677.211107	259514.672655	39.191488
2679.581434	259867.165321	39.196506
2682.045053	260220.202548	39.201524
2685.150891	260582.435918	39.206541
2687.385583	260947.602061	39.211559
2690.088779	261289.654142	39.216576
2692.973946	261662.872477	39.221594
2695.772055	262026.883841	39.226612
2698.552825	262399.764000	39.231629
2701.165166	262764.237518	39.236647
2704.460628	263129.822598	39.241664
2706.742582	263507.025354	39.246682
2709.501298	263864.948353	39.251700
2712.626852	264236.455042	39.256717
2714.954090	264627.140845	39.261735
2718.058855	264994.104453	39.266752
2720.349801	265371.815802	39.271770
2723.232402	265752.482176	39.276788
2725.948040	266141.228141	39.281805
2728.794770	266519.563799	39.286823
2731.808270	266897.822556	39.291840
2734.387910	267284.152344	39.296858
2737.251386	267668.659257	39.301876
2739.992014	268056.259706	39.306893
2742.514211	268444.250672	39.311911
2745.487624	268828.740999	39.316928
2748.151701	269223.213251	39.321946
2750.798321	269608.594125	39.326964
2753.860363	270000.996955	39.331981
2756.538903	270398.211156	39.336999
2759.743608	270782.843782	39.342016
2762.356864	271176.639248	39.347034
2765.544965	271557.896196	39.352052
2768.234213	271954.271090	39.357069
2770.639605	272345.686608	39.362087
2773.337494	272721.636066	39.367104
2776.235419	273125.954950	39.372122
2779.157675	273524.147859	39.377140
2781.826478	273913.184950	39.382157
2784.405069	274312.067510	39.387175
2787.463184	274699.163210	39.392192
2790.217439	275100.939430	39.397210
2792.773478	275499.241386	39.402228
2796.149586	275885.702509	39.407245
2798.716408	276274.730503	39.412263
2801.544539	276628.736589	39.417280
2804.372486	276987.493111	39.422298
2806.998702	277355.579181	39.427316
2809.729573	277704.011790	39.432333
2812.597708	278074.701383	39.437351
2815.120966	278422.684061	39.442368
2817.664325	278796.574928	39.447386
2820.147291	279166.359900	39.452404
2822.918881	279535.463967	39.457421
2825.270408	279928.183331	39.462439
2828.282224	280316.885864	39.467456
2830.986077	280711.962417	39.472474
2833.519125	281107.599288	39.477492
2836.005467	281502.151000	39.482509
2838.689717	281915.926847	39.487527
2841.874392	282329.699403	39.492544
2844.924480	282746.719201	39.497562
2847.508993	283163.024909	39.502580
2850.242264	283575.470857	39.507597
2853.216679	284004.237949	39.512615
2856.059610	284410.873913	39.517632
2858.946931	284863.583806	39.522650
2861.613066	285304.312574	39.527668
2864.798758	285708.047923	39.532685
2867.707513	286162.378822	39.537703
2870.597239	286589.962800	39.542720
2873.525632	287043.527440	39.547738
2876.472551	287474.759355	39.552756
2879.643055	287902.703753	39.557773
2882.416173	288342.827700	39.562791
2885.389230	288799.228032	39.567808
2888.706393	289231.821562	39.572826
2891.607822	289663.692796	39.577844
2894.784624	290110.837656	39.582861
2897.503965	290555.361537	39.587879
2900.683301	290978.245000	39.592896
2903.574437	291420.504818	39.597914
2906.559366	291855.306070	39.602932
2909.639985	292294.181230	39.607949
2912.298954	292733.046144	39.612967
2915.460882	293170.357285	39.617984
2918.359516	293608.039513	39.623002
2921.131240	294057.857908	39.628020
2924.360294	294487.687587	39.633037
2927.232369	294916.480623	39.638055
2930.027648	295367.842096	39.643072
2933.195125	295808.068330	39.648090
2936.361753	296254.085413	39.653108
2939.549876	296681.427597	39.658125
2941.913299	297124.623201	39.663143
2945.077652	297558.774916	39.668160
2948.058691	297985.334078	39.673178
2950.860331	298440.294436	39.678196
2954.129924	298870.590695	39.683213
2957.224567	299294.385364	39.688231
2959.849137	299694.274285	39.693248
2962.641600	300105.947402	39.698266
2965.017206	300498.812185	39.703284
2968.279768	300925.294114	39.708301
2970.511475	301325.977905	39.713319
2973.207399	301727.755665	39.718336
2975.969551	302173.288199	39.723354
2979.014046	302579.961809	39.728372
2981.990950	303025.915078	39.733389
2984.879107	303443.635152	39.738407
2987.768345	303884.240092	39.743424
2990.862830	304339.594488	39.748442
2993.343238	304759.229547	39.753460
2996.725907	305214.637104	39.758477
2999.061682	305676.990807	39.763495
3002.562962	306134.535576	39.768512
3005.246141	306609.912347	39.773530
3008.473475	307073.821932	39.778548
3011.212238	307532.193729	39.783565
3014.079897	308030.853497	39.788583
3017.484355	308487.922673	39.793600
3020.474304	308963.115126	39.798618
3023.392210	309465.520359	39.803636
3026.788037	309916.007001	39.808653
3029.261685	310423.406067	39.813671
3033.021849	310878.352508	39.818688
3036.095030	311375.213333	39.823706
3039.264018	311874.241171	39.828724
3042.475430	312337.929792	39.833741
3045.542811	312844.563735	39.838759
3048.554359	313297.459938	39.843776
3051.651211	313797.887426	39.848794
3054.789468	314301.480857	39.853812
3057.814272	314775.983013	39.858829
3061.256326	315278.761710	39.863847
3064.276430	315768.143577	39.868864
3067.636917	316245.659031	39.873882
3070.690712	316723.703307	39.878900
3074.034172	317206.601258	39.883917
3077.418910	317692.258667	39.888935
3080.311494	318183.706015	39.893952
3083.663699	318653.744101	39.898970
3086.483160	319150.302954	39.903988
3090.069190	319618.496001	39.909005
3092.993826	320100.683627	39.914023
3096.237587	320578.246740	39.919040
3099.495062	321056.465488	39.924058
3102.472159	321543.487958	39.929076
3105.730702	322009.053808	39.934093
3108.654302	322500.269918	39.939111
3111.795041	322979.106238	39.944128
3114.744912	323447.659208	39.949146
3117.572788	323940.075869	39.954164
3121.009657	324417.485856	39.959181
3123.993569	324875.536966	39.964199
3126.884144	325337.841388	39.969216
3130.056779	325777.826670	39.974234
3132.825589	326233.644019	39.979252
3136.151073	326672.330479	39.984269
3138.674899	327117.769496	39.989287
3141.567201	327581.736838	39.994304
3144.702498	328033.092545	39.999322
3147.415323	328500.257180	40.004340
3150.466316	328969.854144	40.009357
3153.469434	329471.351124	40.014375
3156.181335	329928.298632	40.019392
3159.167281	330444.114185	40.024410
3162.103812	330950.893762	40.029428
3165.121640	331448.718410	40.034445
3168.388542	331969.938468	40.039463
3171.416309	332472.376146	40.044480
3174.854985	332983.150426	40.049498
3177.829846	333507.046392	40.054516
3181.048573	334031.534696	40.059533
3184.303779	334570.487053	40.064551
3187.454637	335079.539492	40.069568
3190.441213	335633.812229	40.074586
3193.645800	336180.225224	40.079604
3197.133351	336705.056797	40.084621
3200.253037	337247.411833	40.089639
3203.626911	337827.479145	40.094656
3207.175411	338339.414685	40.099674
3210.003875	338916.968687	40.104692
3213.814576	339442.742841	40.109709
3217.242735	340021.410780	40.114727
3220.454090	340557.375925	40.119744
3223.721204	341092.413630	40.124762
3227.125563	341646.086540	40.129780
3230.311993	342201.388497	40.134797
3233.676944	342741.652064	40.139815
3237.069778	343293.128407	40.144832
3240.673656	343837.406645	40.149850
3243.708118	344389.488143	40.154868
3247.187353	344937.203498	40.159885
3250.694910	345483.563693	40.164903
3253.802144	346030.540623	40.169920
3257.127196	346573.872872	40.174938
3260.115419	347121.340637	40.179956
3263.360404	347688.361461	40.184973
3266.860040	348221.063912	40.189991
3270.017547	348777.831261	40.195008
3273.702752	349322.070208	40.200026
3276.978637	349883.605775	40.205044
3280.094125	350443.561645	40.210061
3283.615630	350982.123552	40.215079
3286.728090	351518.053927	40.220096
3289.815819	352073.377145	40.225114
3293.286990	352632.137048	40.230132
3296.570622	353176.451453	40.235149
3299.662139	353711.347604	40.240167
3302.944248	354238.770573	40.245184
3306.614297	354742.799025	40.250202
3309.239847	355252.851349	40.255220
3312.245827	355749.613675	40.260237
3315.521985	356281.534821	40.265255
3318.529027	356795.750302	40.270272
3321.861119	357319.757555	40.275290
3324.807335	357837.855472	40.280308
3328.083460	358395.441042	40.285325
3331.104414	358919.175983	40.290343
3334.442410	359490.623141	40.295360
3337.987362	360019.847304	40.300378
3340.997968	360585.368722	40.305396
3344.017394	361140.780589	40.310413
3347.592712	361706.656277	40.315431
3350.714473	362274.271995	40.320448
3354.189132	362845.403585	40.325466
3357.632525	363431.405442	40.330484
3361.219860	364011.692221	40.335501
3364.382376	364595.947187	40.340519
3367.478148	365175.332590	40.345536
3371.187196	365758.141185	40.350554
3374.619942	366357.227704	40.355572
3377.655713	366934.975836	40.360589
3381.669039	367567.782407	40.365607
3384.629703	368150.322867	40.370624
3388.494307	368751.313563	40.375642
3391.838669	369360.067185	40.380660
3395.444995	369972.120435	40.385677
3399.149887	370553.699048	40.390695
3402.483653	371183.972235	40.395712
3406.203707	371755.458236	40.400730
3409.739470	372386.493616	40.405748
3412.894077	372963.279744	40.410765
3416.629176	373587.820559	40.415783
3419.798011	374165.932581	40.420800
3423.698244	374806.312482	40.425818
3427.154182	375390.070777	40.430836
3430.684637	376001.794253	40.435853
3433.976978	376599.388778	40.440871
3437.421735	377216.232481	40.445888
3441.171680	377793.642868	40.450906
3444.539595	378426.691993	40.455924
3447.901040	379016.907339	40.460941
3451.649055	379641.073465	40.465959
3455.060180	380233.596653	40.470976
3458.821204	380827.070250	40.475994
3462.373360	381441.217718	40.481012
3466.024614	382059.956696	40.486029
3469.246034	382650.189588	40.491047
3473.005406	383234.874298	40.496064
3476.459838	383876.420004	40.501082
3479.985712	384450.088173	40.506100
3483.343664	385077.854551	40.511117
3486.550967	385644.300774	40.516122
3489.632704	386193.821353	40.521127
3493.123482	386702.149074	40.526132
3495.911961	387134.800886	40.531136
3498.270565	387563.523130	40.536141
3501.603880	387882.284030	40.541146
3503.314971	388202.061418	40.546151
3505.872820	388424.895549	40.551156
3507.883578	388626.607450	40.556160
3509.353869	388826.115103	40.561165
3510.688524	388917.318872	40.566170
3512.386166	388983.519966	40.571175
3513.445676	389070.672896	40.576180
3514.237906	389101.493750	40.581184
3514.786107	389065.324604	40.586189
3515.737324	389071.429608	40.591194
3516.023002	389033.471100	40.596199
3516.924163	388930.776716	40.601204
3517.216341	388882.340582	40.606208
3517.442336	388779.777919	40.611213
3517.823272	388652.321462	40.616218
3517.588411	388571.165510	40.621223
3517.741238	388402.372031	40.626228
3517.783032	388288.368776	40.631232
3517.748581	388177.708384	40.636237
3517.971836	388030.770778	40.641242
3517.057073	387869.950232	40.646247
3517.786164	387709.708287	40.651252
3517.794794	387567.176536	40.656256
3517.443290	387419.488143	40.661261
3516.944109	387243.468687	40.666266
3516.987292	387085.137905	40.671271
3516.746945	386960.621818	40.676276
3516.444863	386761.377051	40.681280
3516.090996	386641.226312	40.686285
3516.032398	386485.858887	40.691290
3515.856103	386317.234911	40.696295
3515.768968	386191.242477	40.701300
3514.925901	386032.742077	40.706304
3515.023680	385871.727248	40.711309
3514.821217	385757.881854	40.716314
3514.383691	385595.602623	40.721319
3514.143476	385490.434198	40.726324
3513.804143	385330.630487	40.731328
3513.869546	385201.024827	40.736333
3513.527689	385092.311021	40.741338
3513.132623	384946.374314	40.746343
3513.096788	384829.626025	40.751348
3512.583950	384721.599371	40.756352
3512.823486	384565.108644	40.761357
3512.767662	384486.839947	40.766362
3512.361831	384387.467495	40.771367
3511.885517	384254.358347	40.776372
3511.987013	384133.084799	40.781376
3511.606988	384017.303917	40.786381
3511.556828	383958.183249	40.791386
3510.990021	383822.289385	40.796391
3511.240412	383727.490900	40.801396
3510.675848	383646.808548	40.806400
3510.799200	383521.409604	40.811405
3510.705368	383461.659259	40.816410
3510.243659	383396.549941	40.821415
3510.142265	383287.131650	40.826420
3510.356392	383176.696742	40.831424
3510.052750	383128.576126	40.836429
3509.824462	383072.152612	40.841434
3509.368434	382969.452719	40.846439
3509.355409	382891.250236	40.851444
3509.212899	382825.224776	40.856448
3508.971169	382780.349285	40.861453
3509.004056	382715.135179	40.866458
3508.703472	382659.866943	40.871463
3508.702383	382586.265240	40.876468
3508.935730	382529.259294	40.881472
3508.569501	382452.459671	40.886477
3508.575158	382380.611360	40.891482
3508.265052	382329.057331	40.896487
3508.352753	382245.700176	40.901492
3508.485461	382167.880095	40.906496
3508.160731	382116.429822	40.911501
3508.211272	382065.428818	40.916506
3507.900021	382042.079725	40.921511
3507.858160	382012.609549	40.926516
3507.642581	381946.390652	40.931520
3507.182219	381875.479780	40.936525
3507.668212	381815.660626	40.941530
3507.369478	381825.652238	40.946535
3507.271482	381773.478968	40.951540
3507.165009	381705.792718	40.956544
3507.165358	381659.631415	40.961549
3507.070845	381648.811836	40.966554
3506.679227	381590.326421	40.971559
3507.153579	381563.266760	40.976564
3507.188896	381549.196601	40.981568
3506.833599	381496.173462	40.986573
3507.100672	381461.160425	40.991578
3506.836013	381434.649861	40.996583
3506.911795	381386.365335	41.001588
3506.309782	381337.882690	41.006592
3506.907874	381284.657684	41.011597
3506.791992	381272.188200	41.016602
3506.250017	381273.265818	41.021607
3506.489256	381229.380683	41.026612
3506.268568	381192.333524	41.031616
3506.275200	381147.365989	41.036621
3506.597963	381106.112602	41.041626
3506.143124	381126.404244	41.046631
3506.425396	381089.786152	41.051636
3506.184485	381051.241471	41.056640
3506.627404	380993.666008	41.061645
3506.495990	380988.345749	41.066650
3506.441555	380981.080361	41.071655
3506.554704	380902.014558	41.076660
3506.222986	380922.286844	41.081664
3506.030202	380862.497207	41.086669
3506.380733	380823.909674	41.091674
3506.034206	380833.222385	41.096679
3506.005206	380823.969112	41.101684
3505.531160	380783.884123	41.106688
3506.070161	380740.154518	41.111693
3506.045303	380730.926002	41.116698
3505.692479	380722.054533	41.121703
3505.995904	380667.247491	41.126708
3505.981617	380693.675586	41.131712
3505.696894	380636.443519	41.136717
3506.017088	380629.958165	41.141722
3506.263836	380587.927790	41.146727
3505.869057	380597.884034	41.151732
3505.722202	380547.904147	41.156736
3505.806910	380562.973133	41.161741
3505.969578	380514.114235	41.166746
3505.617158	380481.945110	41.171751
3505.579798	380474.015643	41.176756
3505.900638	380425.589444	41.181760
3505.647953	380459.711029	41.186765
3505.706065	380431.266635	41.191770
3505.536715	380392.684552	41.196775
3505.997591	380350.747243	41.201780
3505.722093	380382.252791	41.206784
3505.370158	380338.638136	41.211789
3505.797700	380286.710424	41.216794
3505.574193	380318.843659	41.221799
3505.316500	380279.893917	41.226804
3505.888622	380259.074688	41.231808
3505.631429	380245.202898	41.236813
3505.765195	380207.997029	41.241818
3505.290631	380241.797801	41.246823
3505.777862	380193.955431	41.251828
3505.212876	380168.152761	41.256832
3505.296307	380190.826922	41.261837
3505.684681	380136.488953	41.266842
3505.152332	380159.540248	41.271847
3505.098812	380113.080403	41.276852
3505.180199	380121.206535	41.281856
3505.309021	380067.545355	41.286861
3505.440980	380079.707551	41.291866
3505.024362	380080.536475	41.296871
3505.359642	380032.285544	41.301876
3505.087173	380066.766681	41.306880
3505.274319	380014.215316	41.311885
3505.737770	380034.540408	41.316890
3505.357604	379987.699665	41.321895
3505.506894	380006.370333	41.326900
3505.615515	379953.068269	41.331904
3505.576054	379962.815901	41.336909
3505.207035	379941.305941	41.341914
3505.210128	379898.550308	41.346919
3505.442371	379923.235852	41.351924
3505.201183	379878.814709	41.356928
3505.136615	379866.107752	41.361933
3505.487259	379884.059920	41.366938
3505.285524	379855.478140	41.371943
3505.214691	379852.895065	41.376948
3505.150203	379840.696775	41.381952
3505.777801	379801.988128	41.386957
3505.464864	379825.946011	41.391962
3505.058373	379771.733184	41.396967
3505.203910	379783.486374	41.401972
3505.145034	379756.484311	41.406976
3505.003310	379728.350773	41.411981
3505.356785	379748.311881	41.416986
3504.662522	379718.002009	41.421991
3505.098891	379725.792329	41.426996
3505.002538	379711.462538	41.432000
3505.188109	379683.353533	41.437005
3504.990228	379703.757904	41.442010
3504.686715	379693.276030	41.447015
3504.829687	379666.063955	41.452020
3505.001883	379660.110525	41.457024
3504.638013	379657.268545	41.462029
3505.540275	379622.077139	41.467034
3505.405820	379608.134851	41.472039
3505.235847	379582.472827	41.477044
3505.203618	379607.098639	41.482048
3505.090332	379608.973310	41.487053
3504.863789	379561.268431	41.492058
3505.254041	379534.958256	41.497063
3505.250511	379557.061535	41.502068
3505.048513	379561.646299	41.507072
3504.945894	379549.250469	41.512077
3504.847602	379505.721960	41.517082
3505.170478	379512.182228	41.522087
3504.820560	379507.735649	41.527092
3505.209513	379461.968124	41.532096
3505.230511	379497.319022	41.537101
3505.198114	379440.910090	41.542106
3504.924188	379463.107034	41.547111
3505.156008	379441.171170	41.552116
3505.207579	379432.718740	41.557120
3505.127860	379405.160165	41.562125
3505.496275	379425.169946	41.567130
3504.910681	379393.418301	41.572135
3505.026086	379388.440327	41.577140
3505.117010	379376.446238	41.582144
3504.681047	379346.095247	41.587149
3504.797958	379362.151561	41.592154
3504.585808	379331.078440	41.597159
3504.573138	379351.275673	41.602164
3504.868519	379308.651235	41.607168
3504.689204	379354.487615	41.612173
3504.968203	379316.520333	41.617178
3505.038497	379290.413181	41.622183
3504.938353	379329.089901	41.627188
3505.182557	379286.498964	41.632192
3505.110311	379244.466700	41.637197
3505.125985	379254.485575	41.642202
3504.879267	379256.254181	41.647207
3504.947299	379215.929278	41.652212
3504.793353	379256.725666	41.657216
3504.803756	379238.182083	41.662221
3504.890327	379208.206211	41.667226
3504.902104	379202.074591	41.672231
3505.018205	379206.125851	41.677236
3504.759498	379178.798891	41.682240
3504.965611	379159.893681	41.687245
3505.051993	379192.589290	41.692250
3504.785261	379191.283446	41.697255
3504.529242	379142.870541	41.702260
3505.328467	379115.706956	41.707264
3505.000115	379124.584807	41.712269
3504.857773	379144.650035	41.717274
3504.823530	379135.778713	41.722279
3505.080733	379081.053057	41.727284
3504.974845	379092.515546	41.732288
3504.959845	379079.062886	41.737293
3504.982378	379079.949584	41.742298
3504.613626	379081.355965	41.747303
3504.728281	379054.198812	41.752308
3504.873554	379054.379366	41.757312
3504.776626	379052.894065	41.762317
3504.758980	379025.808676	41.767322
3504.838727	379038.310104	41.772327
3504.898964	379021.767902	41.777332
3504.982066	379018.473694	41.782336
3504.884628	378993.817218	41.787341
3505.027592	378984.892415	41.792346
3504.676924	378994.816657	41.797351
3504.825763	378963.126612	41.802356
3504.632184	378976.383446	41.807360
3505.018128	378941.476529	41.812365
3504.864146	378954.599936	41.817370
3504.449377	378930.578587	41.822375
3504.753422	378933.430155	41.827380
3504.442395	378944.416414	41.832384
3504.223975	378907.722813	41.837389
3504.569090	378914.510320	41.842394
3504.514116	378953.434619	41.847399
3504.750667	378921.806980	41.852404
3504.942160	378891.025796	41.857408
3504.774167	378915.927853	41.862413
3504.718314	378923.414617	41.867418
3504.809193	378902.034867	41.872423
3504.832004	378859.020633	41.877428
3505.249489	378838.708363	41.882432
3504.929571	378867.576902	41.887437
3505.006596	378862.147098	41.892442
3504.802103	378833.336093	41.897447
3504.736698	378816.228659	41.902452
3504.767204	378835.910630	41.907456
3505.013762	378800.466051	41.912461
3505.067680	378802.950206	41.917466
3504.641096	378810.063199	41.922471
3505.042426	378770.117550	41.927476
3504.859070	378779.226909	41.932480
3504.800042	378755.607051	41.937485
3505.204051	378751.931437	41.942490
3504.832215	378734.694361	41.947495
3505.278215	378720.329346	41.952500
3505.088930	378696.831784	41.957504
3505.071825	378707.364684	41.962509
3505.009454	378672.426657	41.967514
3505.220332	378680.329137	41.972519
3505.158935	378657.777872	41.977524
3505.085714	378653.770725	41.982528
3504.729013	378637.548622	41.987533
3504.942499	378598.649902	41.992538
3504.742327	378623.786146	41.997543
3504.796981	378581.046364	42.002548
3504.733608	378613.791562	42.007552
3504.664351	378567.230633	42.012557
3504.746566	378595.527098	42.017562
3505.054149	378574.112915	42.022567
3504.671010	378572.113264	42.027572
3505.010436	378550.973822	42.032576
3504.503735	378545.254718	42.037581
3504.933487	378543.533531	42.042586
3504.709812	378522.991793	42.047591
3504.683764	378543.293296	42.052596
3504.966411	378513.031548	42.057600
3504.565358	378493.433504	42.062605
3504.844829	378510.202092	42.067610
3504.561039	378518.360847	42.072615
3504.540458	378481.228611	42.077620
3504.781695	378484.090140	42.082624
3504.548394	378487.586259	42.087629
3504.615437	378482.157980	42.092634
3504.799427	378440.058919	42.097639
3504.655072	378479.557391	42.102644
3504.487802	378461.143270	42.107648
3504.749980	378431.647755	42.112653
3504.916708	378424.524978	42.117658
3504.726143	378454.009255	42.122663
3504.830106	378420.367349	42.127668
3504.839728	378401.747190	42.132672
3504.551230	378418.300376	42.137677
3504.943548	378399.568850	42.142682
3504.577982	378388.587730	42.147687
3504.909730	378371.519064	42.152692
3504.679514	378396.176930	42.157696
3504.719176	378359.136798	42.162701
3504.710415	378337.492704	42.167706
3504.314625	378359.073648	42.172711
3504.601299	378334.050816	42.177716
3504.651136	378340.198343	42.182720
3504.477505	378339.615379	42.187725
3504.518799	378296.953708	42.192730
3504.883645	378331.818893	42.197735
3504.991293	378299.524378	42.202740
3504.738869	378292.925674	42.207744
3504.760722	378293.583579	42.212749
3504.938919	378279.794881	42.217754
3504.369367	378267.853990	42.222759
3504.660605	378269.944568	42.227764
3504.941987	378267.432889	42.232768
3504.179907	378255.446122	42.237773
3504.537037	378228.275508	42.242778
3504.422802	378236.000550	42.247783
3504.249408	378243.251669	42.252788
3504.637976	378242.172865	42.257792
3504.788835	378228.846310	42.262797
3504.793588	378217.603119	42.267802
3504.337662	378229.477287	42.272807
3504.697678	378209.275521	42.277812
3504.891158	378224.633437	42.282816
3504.668537	378194.934591	42.287821
3505.040049	378174.959910	42.292826
3504.905608	378192.506257	42.297831
3504.798268	378168.359540	42.302836
3504.911002	378164.907965	42.307840
3504.600628	378164.194001	42.312845
3504.617619	378137.560367	42.317850
3504.339438	378125.878601	42.322855
3504.936736	378125.504430	42.327860
3504.869873	378121.318175	42.332864
3504.543258	378109.923850	42.337869
3504.489878	378113.035463	42.342874
3504.623841	378109.555092	42.347879
3504.760792	378093.356473	42.352884
3504.956778	378079.081618	42.357888
3504.726163	378064.645273	42.362893
3505.019086	378068.592392	42.367898
3504.307370	378064.736987	42.372903
3504.448846	378037.269670	42.377908
3504.842214	378051.604067	42.382912
3504.989952	378045.527083	42.387917
3504.924210	378026.409950	42.392922
3504.952072	378023.633104	42.397927
3504.752379	378002.044445	42.402932
3504.692086	377984.121904	42.407936
3504.500645	378001.702781	42.412941
3505.221113	377964.681840	42.417946
3504.543924	377976.565624	42.422951
3504.752959	377961.423853	42.427956
3504.925331	377950.789981	42.432960
3504.729351	377934.287826	42.437965
3504.661341	377924.276966	42.442970
3504.249572	377936.042499	42.447975
3504.246931	377917.729279	42.452980
3504.772006	377917.137602	42.457984
3504.217319	377923.635111	42.462989
3504.857175	377887.135554	42.467994
3504.637664	377899.353984	42.472999
3504.133882	377912.533031	42.478004
3504.581575	377889.926290	42.483008
3504.270448	377879.012729	42.488013
3504.314045	377885.161312	42.493018
3504.669668	377867.834300	42.498023
3504.442483	377886.641792	42.503028
3504.596418	377862.351845	42.508032
3504.466881	377861.126011	42.513037
3504.668161	377848.910529	42.518042
3504.321843	377830.193754	42.523047
3504.187850	377864.705798	42.528052
3504.834028	377847.612639	42.533056
3504.576457	377839.361351	42.538061
3505.126608	377807.708687	42.543066
3504.447644	377841.187726	42.548071
3504.480054	377815.136461	42.553076
3504.469608	377805.498007	42.558080
3504.502195	377794.301168	42.563085
3504.188411	377799.387086	42.568090
3504.920220	377774.166358	42.573095
3504.498246	377800.762587	42.578100
3504.948736	377789.041842	42.583104
3504.545279	377757.336396	42.588109
3504.479971	377774.108926	42.593114
3504.316813	377783.495114	42.598119
3504.514655	377742.461425	42.603124
3504.581449	377750.641225	42.608128
3504.262940	377744.612462	42.613133
3504.522867	377732.387673	42.618138
3504.676872	377743.911212	42.623143
3504.493614	377733.969393	42.628148
3504.724211	377746.650869	42.633152
3504.778903	377725.276205	42.638157
3504.569185	377713.837853	42.643162
3504.270840	377704.982523	42.648167
3504.470169	377696.353751	42.653172
3504.647757	377703.651228	42.658176
3504.525542	377688.180179	42.663181
3504.320990	377700.421741	42.668186
3504.678334	377701.280981	42.673191
3504.581160	377674.334419	42.678196
3504.739099	377681.787622	42.683200
3504.673985	377666.129487	42.688205
3504.836564	377662.771732	42.693210
3504.654866	377628.411238	42.698215
3504.473016	377644.693528	42.703220
3504.741164	377637.656321	42.708224
3504.290838	377620.253117	42.713229
3504.438116	377618.652851	42.718234
3504.442874	377614.963938	42.723239
3504.480606	377619.918004	42.728244
3504.752419	377614.889647	42.733248
3504.693431	377606.963022	42.738253
3504.528287	377592.261798	42.743258
3504.367603	377607.981168	42.748263
3504.318338	377593.515985	42.753268
3504.774798	377576.529008	42.758272
3504.599687	377573.148319	42.763277
3504.799997	377561.772287	42.768282
3504.536688	377553.394667	42.773287
3504.554627	377565.651971	42.778292
3504.586858	377541.762606	42.783296
3504.351662	377509.063799	42.788301
3504.458869	377536.670298	42.793306
3504.257488	377508.188506	42.798311
3504.029251	377544.343624	42.803316
3504.467669	377520.033934	42.808321
3504.365626	377539.534013	42.813325
3504.529879	377506.543137	42.818330
3504.372082	377523.559317	42.823335
3504.545158	377503.666539	42.828340
3504.641666	377500.853370	42.833345
3504.161398	377518.734476	42.838349
3504.454473	377505.436069	42.843354
3504.393066	377484.791835	42.848359
3504.461018	377469.163461	42.853364
3504.527472	377484.160203	42.858369
3504.293399	377480.636211	42.863373
3504.194382	377461.524067	42.868378
3504.391188	377496.416549	42.873383
3504.490073	377438.330674	42.878388
3504.525983	377466.838751	42.883393
3504.634007	377444.056528	42.888397
3504.281055	377463.748923	42.893402
3504.391294	377457.143622	42.898407
3504.083937	377453.122493	42.903412
3504.466655	377403.563619	42.908417
3504.364158	377423.750598	42.913421
3504.097074	377423.614805	42.918426
3504.549325	377428.757729	42.923431
3504.370470	377417.187232	42.928436
3504.632604	377433.755528	42.933441
3504.427598	377413.286573	42.938445
3504.549211	377393.859724	42.943450
3504.545281	377410.266600	42.948455
3504.433065	377414.303264	42.953460
3504.709929	377404.771912	42.958465
3504.729573	377393.653315	42.963469
3504.425684	377374.293719	42.968474
3504.483276	377380.033192	42.973479
3504.286177	377372.789688	42.978484
3504.328242	377387.561398	42.983489
3504.644177	377374.284770	42.988493
3504.875897	377349.346315	42.993498
3504.592857	377346.287900	42.998503
3504.239534	377372.212225	43.003508
3504.768293	377345.242804	43.008513
3504.572136	377319.558014	43.013517
3504.759099	377328.405678	43.018522
3504.475753	377326.441060	43.023527
3504.854153	377317.453230	43.028532
3504.595396	377293.355355	43.033537
3504.294956	377312.251005	43.038541
3504.519888	377303.897897	43.043546
3504.598742	377301.367301	43.048551
3504.386448	377289.420512	43.053556
3504.499928	377264.042846	43.058561
3504.312457	377260.486032	43.063565
3504.607540	377273.132029	43.068570
3504.287538	377277.557657	43.073575
3504.471859	377263.309791	43.078580
3504.580191	377241.951826	43.083585
3504.542025	377246.587267	43.088589
3504.806134	377230.546249	43.093594
3504.640481	377228.588458	43.098599
3504.305401	377214.270063	43.103604
3504.863924	377195.766061	43.108609
3504.565859	377204.130829	43.113613
3504.623080	377202.239549	43.118618
3504.458139	377195.423344	43.123623
3504.769260	377177.467164	43.128628
3504.875795	377178.366063	43.133633
3504.517789	377186.180715	43.138637
3504.584611	377150.839388	43.143642
3504.463455	377141.955923	43.148647
3504.257692	377159.183329	43.153652
3504.330817	377146.428295	43.158657
3504.172904	377144.087734	43.163661
3504.382728	377149.803175	43.168666
3504.502939	377139.431695	43.173671
3504.056329	377115.770386	43.178676
3504.359653	377113.407784	43.183681
3504.331743	377139.051894	43.188685
3504.453406	377119.548596	43.193690
3504.207013	377112.007603	43.198695
3504.258991	377135.705937	43.203700
3504.805428	377121.019235	43.208705
3504.444691	377101.465004	43.213709
3504.373481	377092.522761	43.218714
3504.634919	377091.871003	43.223719
3504.323499	377102.196490	43.228724
3504.656019	377086.475272	43.233729
3504.417463	377081.552962	43.238733
3504.537554	377060.650893	43.243738
3504.538805	377064.796836	43.248743
3504.628278	377072.642519	43.253748
3504.568623	377059.425159	43.258753
3504.551458	377041.062962	43.263757
3505.008996	377027.484037	43.268762
3504.776004	377040.595127	43.273767
3504.579180	377015.291792	43.278772
3504.730862	376995.046037	43.283777
3504.338856	377024.130797	43.288781
3504.543848	376989.276210	43.293786
3504.303550	376980.691343	43.298791
3504.287075	376983.339357	43.303796
3504.392738	376968.544222	43.308801
3504.467329	376974.993282	43.313805
3504.187833	376980.429990	43.318810
3504.674248	376970.356685	43.323815
3504.349383	376964.506863	43.328820
3504.867659	376951.528782	43.333825
3504.559415	376953.892248	43.338829
3504.545515	376943.185809	43.343834
3504.597114	376946.662462	43.348839
3504.255100	376928.987471	43.353844
3504.552049	376916.120674	43.358849
3504.668739	376918.645897	43.363853
3504.684844	376906.586581	43.368858
3504.620552	376914.889019	43.373863
3504.465176	376899.880760	43.378868
3504.302176	376885.713100	43.383873
3504.571851	376895.895909	43.388877
3504.259419	376892.002707	43.393882
3504.427828	376887.372150	43.398887
3504.219796	376877.790143	43.403892
3504.418457	376863.870541	43.408897
3504.332179	376865.156035	43.413901
3504.516929	376857.190731	43.418906
3504.252638	376862.904851	43.423911
3504.315649	376861.063513	43.428916
3504.401409	376863.822556	43.433921
3504.320111	376853.152183	43.438925
3503.973349	376839.522282	43.443930
3503.917339	376856.700708	43.448935
3504.298651	376847.076405	43.453940
3504.449827	376844.610656	43.458945
3504.340140	376846.077906	43.463949
3504.352323	376852.562286	43.468954
3504.404306	376864.280260	43.473959
3504.192178	376855.233058	43.478964
3504.640309	376856.535820	43.483969
3504.361687	376835.442298	43.488973
3504.266910	376830.700720	43.493978
3504.486176	376826.519971	43.498983
3504.350206	376830.000848	43.503988
3504.146529	376815.712412	43.508993
3504.186580	376836.055207	43.513997
3504.504827	376833.766539	43.519002
3504.163222	376803.500431	43.524007
3503.975136	376788.904283	43.529012
3504.733787	376809.336989	43.534017
3504.272251	376794.427961	43.539021
3504.233781	376797.003155	43.544026
3504.160251	376814.260678	43.549031
3504.324203	376811.970963	43.554036
3504.550515	376800.895841	43.559041
3504.252997	376787.639683	43.564045
3504.562677	376771.235170	43.569050
3504.269631	376780.820179	43.574055
3504.187066	376773.329534	43.579060
3504.484008	376758.580395	43.584065
3504.142636	376792.235871	43.589069
3504.437835	376757.443133	43.594074
3504.507206	376774.321974	43.599079
3504.486164	376758.681954	43.604084
3504.157549	376754.104513	43.609089
3504.117916	376764.743233	43.614093
3504.434612	376754.722140	43.619098
3504.517554	376752.928519	43.624103
3504.294265	376751.971834	43.629108
3504.521207	376741.201833	43.634113
3504.466711	376741.592033	43.639117
3504.034932	376716.885251	43.644122
3504.510853	376730.901837	43.649127
3504.183287	376731.665876	43.654132
3504.520681	376724.312327	43.659137
3504.641359	376727.727206	43.664141
3504.357809	376707.168560	43.669146
3504.754926	376700.695842	43.674151
3504.277584	376691.461599	43.679156
3504.591941	376683.094227	43.684161
3504.334481	376695.471640	43.689165
3504.361957	376665.554068	43.694170
3504.153940	376664.773023	43.699175
3504.083571	376657.076936	43.704180
3504.291277	376663.479567	43.709185
3504.321491	376659.659360	43.714189
3504.396739	376670.152762	43.719194
3504.596060	376676.658462	43.724199
3504.243014	376659.315770	43.729204
3504.713799	376642.046334	43.734209
3504.497587	376645.489038	43.739213
3504.671626	376634.218642	43.744218
3504.607510	376635.322585	43.749223
3504.465203	376616.267754	43.754228
3504.783080	376606.348183	43.759233
3504.400856	376610.529355	43.764237
3504.409744	376600.582317	43.769242
3504.644534	376596.195599	43.774247
3504.446487	376589.130159	43.779252
3504.672571	376577.139297	43.784257
3504.421863	376581.808413	43.789261
3504.585376	376575.143673	43.794266
3504.489797	376565.314886	43.799271
3504.423895	376550.851957	43.804276
3504.635756	376535.836384	43.809281
3504.275453	376543.982198	43.814285
3504.490981	376541.684315	43.819290
3504.403854	376534.804824	43.824295
3504.171710	376523.318803	43.829300
3504.302549	376524.569986	43.834305
3504.424118	376515.291902	43.839309
3504.357178	376507.442626	43.844314
3504.465320	376520.398214	43.849319
3504.182641	376526.878385	43.854324
3504.646851	376504.446309	43.859329
3504.256804	376492.756312	43.864333
3504.390293	376484.951657	43.869338
3504.522109	376489.763808	43.874343
3504.204903	376488.694780	43.879348
3504.309214	376488.551147	43.884353
3503.991387	376488.423371	43.889357
3503.862777	376482.644200	43.894362
3504.118734	376488.403317	43.899367
3504.034208	376488.925449	43.904372
3504.480837	376476.747075	43.909377
3504.244875	376480.498154	43.914381
3504.110199	376462.484944	43.919386
3504.719826	376461.065912	43.924391
3504.403673	376464.702486	43.929396
3504.498731	376462.194712	43.934401
3504.207182	376460.689206	43.939405
3504.430976	376461.620458	43.944410
3504.016435	376442.303340	43.949415
3503.710684	376442.784133	43.954420
3504.341754	376435.969150	43.959425
3504.187563	376439.961673	43.964429
3504.198101	376426.885630	43.969434
3504.428790	376415.479035	43.974439
3504.141220	376441.342692	43.979444
3504.343453	376430.830880	43.984449
3504.306858	376434.346955	43.989453
3504.224085	376436.623936	43.994458
3504.136131	376431.626867	43.999463
3504.060601	376427.340058	44.004468
3504.300075	376415.855764	44.009473
3504.114453	376417.691145	44.014477
3504.014724	376414.781737	44.019482
3503.806209	376416.646174	44.024487
3504.043508	376415.387743	44.029492
3504.259658	376420.339190	44.034497
3504.103000	376430.589511	44.039501
3504.211794	376423.653594	44.044506
3504.496286	376426.508434	44.049511
3504.297274	376422.164835	44.054516
3504.284729	376421.378321	44.059521
3504.390088	376432.248575	44.064525
3504.368395	376414.446413	44.069530
3504.541018	376397.758174	44.074535
3504.371524	376384.608829	44.079540
3504.329587	376393.696376	44.084545
3504.365907	376398.269267	44.089549
3504.463684	376397.312694	44.094554
3504.429851	376384.040157	44.099559
3504.106325	376379.945165	44.104564
3504.326367	376368.285873	44.109569
3504.161982	376368.820631	44.114573
3504.349777	376374.514228	44.119578
3504.209202	376369.220230	44.124583
3504.317826	376373.883440	44.129588
3504.367678	376377.487602	44.134593
3504.328073	376372.330262	44.139597
3504.402375	376346.449478	44.144602
3504.258344	376345.760058	44.149607
3504.476904	376348.320086	44.154612
3504.229124	376339.100348	44.159617
3504.236632	376337.547563	44.164621
3504.267537	376337.720772	44.169626
3504.348846	376339.030665	44.174631
3504.174021	376332.699172	44.179636
3504.184060	376322.268587	44.184641
3504.268968	376320.016776	44.189645
3504.060977	376320.456680	44.194650
3504.124621	376315.766308	44.199655
3503.815640	376319.249142	44.204660
3504.093681	376335.026840	44.209665
3504.081477	376321.750864	44.214669
3504.203111	376323.715736	44.219674
3504.149710	376319.298234	44.224679
3504.348607	376335.266500	44.229684
3504.340870	376331.604880	44.234689
3504.210347	376323.053393	44.239693
3504.448090	376325.534080	44.244698
3504.206944	376308.784029	44.249703
3503.762006	376300.867282	44.254708
3504.018821	376288.311870	44.259713
3504.208938	376298.049547	44.264717
3503.983014	376295.414446	44.269722
3504.317943	376299.355100	44.274727
3504.202978	376306.928009	44.279732
3504.185306	376298.155183	44.284737
3504.177597	376312.095746	44.289741
3504.411646	376306.310095	44.294746
3504.790670	376312.126093	44.299751
3504.286884	376293.179125	44.304756
3504.573557	376284.536243	44.309761
3504.484757	376276.410573	44.314765
3504.481984	376269.008968	44.319770
3504.584492	376281.049801	44.324775
3504.608211	376270.057433	44.329780
3504.496244	376240.950127	44.334785
3503.987576	376248.305478	44.339789
3504.276417	376247.089768	44.344794
3504.488325	376226.961291	44.349799
3504.161697	376248.990298	44.354804
3504.129437	376250.979500	44.359809
3504.645948	376254.535341	44.364813
3504.247886	376231.043894	44.369818
3504.163918	376224.418218	44.374823
3504.170420	376226.910029	44.379828
3504.511589	376211.314287	44.384833
3504.196810	376221.691403	44.389837
3504.017947	376222.737185	44.394842
3504.526612	376216.755491	44.399847
3504.205673	376225.124077	44.404852
3504.381033	376218.152165	44.409857
3504.179869	376198.165281	44.414861
3504.084003	376197.595429	44.419866
3504.322357	376189.697831	44.424871
3504.179333	376207.017472	44.429876
3504.391330	376194.316495	44.434881
3504.471487	376201.782269	44.439885
3504.387383	376198.514261	44.444890
3504.211187	376204.341732	44.449895
3504.061335	376184.117799	44.454900
3504.251272	376176.482219	44.459905
3504.076576	376168.064865	44.464909
3504.203355	376166.645840	44.469914
3504.285393	376171.262403	44.474919
3504.037255	376172.039333	44.479924
3504.365300	376166.874724	44.484929
3504.369524	376174.708621	44.489933
3504.232223	376172.644548	44.494938
3504.646270	376166.983045	44.499943
3504.038650	376156.650055	44.504948
3504.226748	376142.350323	44.509953
3504.163877	376138.417597	44.514957
3504.346867	376146.350425	44.519962
3504.362241	376142.329020	44.524967
3504.136266	376159.305679	44.529972
3504.351276	376148.969832	44.534977
3504.502610	376150.675650	44.539981
3504.550884	376123.272630	44.544986
3504.613617	376134.454944	44.549991
3504.221712	376127.470940	44.554996
3504.425743	376108.564616	44.560001
3504.651134	376125.978675	44.565005
3504.628091	376105.810968	44.570010
3504.519700	376090.820418	44.575015
3504.365079	376091.684313	44.580020
3504.862659	376075.402436	44.585025
3504.707145	376086.441205	44.590029
3504.417744	376065.298110	44.595034
3504.350404	376049.232708	44.600039
3504.107639	376050.059665	44.605044
3504.209377	376054.444195	44.610049
3504.284752	376052.143002	44.615053
3504.702998	376056.502937	44.620058
3504.389898	376036.609978	44.625063
3504.468624	376030.492726	44.630068
3504.709816	376012.623394	44.635073
3504.583679	376018.849968	44.640077
3504.303621	376015.689232	44.645082
3504.507601	376010.722273	44.650087
3504.492907	375993.656489	44.655092
3504.194207	376011.178881	44.660097
3504.232759	376004.177684	44.665101
3504.029932	375998.054060	44.670106
3504.066431	376000.464833	44.675111
3503.791807	376014.905555	44.680116
3504.397021	376000.005661	44.685121
3503.907538	376001.609289	44.690125
3503.935504	376011.906841	44.695130
3504.319473	376019.680739	44.700135
3504.435529	376003.001280	44.705140
3504.592848	376016.432556	44.710145
3504.782545	375999.080096	44.715149
3504.532835	375965.059610	44.720154
3504.680405	375989.481177	44.725159
3504.519591	375954.988767	44.730164
3504.452368	375952.608362	44.735169
3504.581131	375945.033283	44.740173
3504.424721	375947.347369	44.745178
3504.581858	375938.368773	44.750183
3504.331517	375929.251093	44.755188
3504.552227	375917.210012	44.760193
3504.354801	375909.203188	44.765197
3504.299150	375894.331413	44.770202
3504.334290	375915.184187	44.775207
3504.311122	375896.466301	44.780212
3504.307143	375909.795926	44.785217
3504.516247	375902.106391	44.790221
3504.001685	375879.955877	44.795226
3504.825573	375849.428504	44.800231
3504.438148	375899.931275	44.805236
3504.322601	375868.687564	44.810241
3504.049425	375894.167740	44.815245
3504.117794	375859.003096	44.820250
3504.333590	375892.215126	44.825255
3504.342319	375875.578018	44.830260
3504.113868	375847.786128	44.835265
3504.423402	375849.873942	44.840269
3504.123843	375849.794149	44.845274
3504.261766	375851.654721	44.850279
3504.054159	375832.609843	44.855284
3504.302029	375860.703995	44.860289
3504.303637	375838.471863	44.865293
3504.206993	375870.588637	44.870298
3504.103890	375839.393810	44.875303
3503.950649	375857.071334	44.880308
3504.086731	375835.886297	44.885313
3504.159255	375851.137058	44.890317
3504.392892	375816.989168	44.895322
3504.373205	375811.268994	44.900327
3503.922041	375831.689945	44.905332
3504.233015	375824.035166	44.910337
3504.048488	375823.581071	44.915341
3504.163422	375827.505675	44.920346
3504.640972	375822.037582	44.925351
3504.148558	375840.684460	44.930356
3504.506926	375817.302131	44.935361
3504.540880	375814.117178	44.940365
3504.469532	375806.014092	44.945370
3504.583890	375795.058141	44.950375
3504.312090	375796.398432	44.955380
3504.488222	375802.119392	44.960385
3504.814642	375782.405022	44.965389
3504.389246	375778.275198	44.970394
3504.786633	375770.759371	44.975399
3504.498571	375767.752503	44.980404
3504.660805	375752.312055	44.985409
3504.495334	375728.656364	44.990413
3504.308726	375731.356792	44.995418
3504.209244	375726.183398	45.000423
3504.108391	375733.169131	45.005428
3504.548355	375719.745169	45.010433
3504.370635	375713.388599	45.015437
3504.327642	375704.543336	45.020442
3504.358316	375704.436778	45.025447
3504.329312	375693.299965	45.030452
3504.395869	375691.127331	45.035457
3504.300580	375680.229927	45.040461
3504.437372	375701.448298	45.045466
3504.690041	375681.313108	45.050471
3504.377991	375666.761588	45.055476
3504.624940	375657.183680	45.060481
3504.317322	375655.451749	45.065485
3504.336376	375656.568008	45.070490
3504.526007	375650.026173	45.075495
3504.417617	375635.035455	45.080500
3504.314638	375627.598698	45.085505
3504.238814	375636.361089	45.090509
3504.166456	375638.611031	45.095514
3504.544583	375630.029865	45.100519
3504.375021	375642.190208	45.105524
3504.471478	375625.590003	45.110529
3504.255326	375608.148909	45.115533
3504.172278	375606.432351	45.120538
3504.256341	375589.706906	45.125543
3504.099299	375594.870071	45.130548
3504.301372	375605.394575	45.135553
3504.522198	375576.793802	45.140557
3504.387374	375605.635428	45.145562
3504.465448	375577.820336	45.150567
3503.917353	375573.709887	45.155572
3504.476974	375559.834526	45.160577
3504.237245	375570.556064	45.165581
3504.024997	375576.185827	45.170586
3504.522409	375576.539667	45.175591
3504.432662	375584.973587	45.180596
3504.257702	375570.654733	45.185601
3504.206064	375557.893484	45.190605
3504.497114	375568.454807	45.195610
3504.403946	375542.371049	45.200615
3504.011797	375545.841658	45.205620
3504.313542	375526.334562	45.210625
3504.147807	375546.557912	45.215629
3504.282571	375542.492138	45.220634
3504.485067	375535.363197	45.225639
3504.314968	375542.665154	45.230644
3504.102671	375534.507984	45.235649
3504.200445	375522.842340	45.240653
3503.820297	375506.241117	45.245658
3504.205513	375516.533196	45.250663
3503.851332	375528.010516	45.255668
3503.966229	375504.895430	45.260673
3503.877027	375533.297463	45.265677
3503.880499	375500.050555	45.270682
3503.980376	375534.349564	45.275687
3504.250732	375513.880812	45.280692
3504.157155	375533.787516	45.285697
3504.119479	375514.995436	45.290701
3504.111978	375533.031619	45.295706
3504.538907	375537.466549	45.300711
3504.002228	375533.074483	45.305716
3504.276704	375524.636865	45.310721
3504.218387	375527.037217	45.315725
3504.087971	375544.787579	45.320730
3504.151205	375536.307045	45.325735
3504.125067	375540.991654	45.330740
3504.120435	375530.105316	45.335745
3504.087534	375514.161444	45.340749
3504.031822	375509.464410	45.345754
3504.052771	375496.996914	45.350759
3503.796903	375510.748045	45.355764
3504.090522	375506.072101	45.360769
3504.317122	375515.982259	45.365773
3503.973272	375513.696431	45.370778
3504.475305	375506.418386	45.375783
3504.073862	375517.038316	45.380788
3504.347074	375502.953838	45.385793
3504.530615	375505.010713	45.390797
3504.248599	375523.090295	45.395802
3504.313520	375510.793912	45.400807
3504.228701	375507.347901	45.405812
3504.314683	375481.413845	45.410817
3504.340176	375479.705561	45.415821
3504.137022	375481.009574	45.420826
3504.218060	375477.689965	45.425831
3503.958872	375484.497272	45.430836
3504.023914	375479.577649	45.435841
3504.029900	375498.603766	45.440845
3504.363155	375487.435070	45.445850
3504.460902	375485.893424	45.450855
3504.252319	375499.204652	45.455860
3504.488309	375480.394733	45.460865
3504.366162	375456.630287	45.465869
3504.302671	375461.829554	45.470874
3504.306311	375442.191481	45.475879
3504.466480	375451.934096	45.480884
3504.375591	375470.288735	45.485889
3504.011979	375448.164998	45.490893
3504.306788	375444.837032	45.495898
3504.349823	375439.234077	45.500903
3504.009238	375436.413548	45.505908
3504.553180	375423.608983	45.510913
3504.222409	375423.559560	45.515917
3504.168272	375430.970393	45.520922
3504.449602	375425.380641	45.525927
3504.310689	375431.431264	45.530932
3504.556239	375416.409952	45.535937
3504.345777	375407.362163	45.540941
3504.395038	375401.147724	45.545946
3504.842300	375394.310751	45.550951
3504.222656	375383.292657	45.555956
3504.507776	375392.125230	45.560961
3504.460330	375368.603296	45.565965
3503.963495	375361.813808	45.570970
3503.893154	375357.856750	45.575975
3503.857679	375365.976889	45.580980
3504.408340	375356.223714	45.585985
3504.437707	375368.810563	45.590989
3504.427588	375365.607104	45.595994
3504.600043	375363.036154	45.600999
3504.307249	375350.185774	45.606004
3504.353263	375336.289779	45.611009
3504.561371	375328.218734	45.616013
3504.433795	375316.461468	45.621018
3504.318559	375319.405013	45.626023
3504.181867	375343.515781	45.631028
3504.710208	375321.581662	45.636033
3504.466024	375301.245015	45.641037
3504.238054	375290.368480	45.646042
3504.486350	375300.173512	45.651047
3504.062191	375303.623763	45.656052
3504.176977	375298.950628	45.661057
3504.378267	375306.880727	45.666061
3504.427682	375297.283086	45.671066
3504.260771	375275.179035	45.676071
3504.252330	375272.585800	45.681076
3504.278503	375262.915513	45.686081
3504.365893	375260.052755	45.691085
3504.415169	375265.157909	45.696090
3504.474774	375265.326587	45.701095
3504.531934	375259.746812	45.706100
3504.280287	375238.114009	45.711105
3504.069219	375233.136253	45.716109
3504.225741	375215.636080	45.721114
3504.348076	375222.840992	45.726119
3504.154030	375245.002207	45.731124
3504.281542	375218.527235	45.736129
3504.247528	375254.679134	45.741133
3504.196978	375232.709291	45.746138
3504.294517	375235.263084	45.751143
3504.354923	375240.519106	45.756148
3504.172015	375206.105866	45.761153
3504.227063	375208.768127	45.766157
3504.448103	375202.526504	45.771162
3504.525666	375198.800425	45.776167
3504.271566	375211.762818	45.781172
3504.387065	375199.076785	45.786177
3504.345492	375203.204251	45.791181
3503.861965	375185.703492	45.796186
3504.162237	375170.317316	45.801191
3503.872487	375166.089675	45.806196
3503.796139	375170.604202	45.811201
3503.833010	375191.355324	45.816205
3503.703036	375202.135921	45.821210
3504.164137	375206.463736	45.826215
3504.172666	375214.704135	45.831220
3504.146507	375203.668488	45.836225
3504.110323	375199.629704	45.841229
3503.859602	375192.979344	45.846234
3504.379767	375172.089371	45.851239
3504.351962	375177.410220	45.856244
3504.440384	375185.587121	45.861249
3504.187441	375188.603319	45.866253
3504.095608	375186.964444	45.871258
3504.346051	375177.131497	45.876263
3504.122353	375191.920583	45.881268
3504.293209	375186.729824	45.886273
3503.988303	375179.630155	45.891277
3503.585036	375178.523821	45.896282
3504.170264	375183.188140	45.901287
3504.129876	375194.972073	45.906292
3504.106468	375191.109329	45.911297
3504.067067	375166.110639	45.916301
3503.916861	375157.765516	45.921306
3504.307759	375155.668770	45.926311
3504.178702	375154.976962	45.931316
3504.005365	375155.843836	45.936321
3504.312826	375148.469298	45.941325
3504.078602	375154.000842	45.946330
3504.177143	375153.145869	45.951335
3504.434520	375166.205486	45.956340
3504.282090	375162.490322	45.961345
3504.212280	375161.509337	45.966349
3504.183009	375158.970262	45.971354
3504.512805	375147.369584	45.976359
3503.967644	375142.597254	45.981364
3504.147298	375129.748434	45.986369
3504.046027	375131.697725	45.991373
3504.078069	375136.449497	45.996378
3504.170958	375126.514257	46.001383
3504.436167	375126.446934	46.006388
3504.269393	375128.711829	46.011393
3504.124917	375127.437398	46.016397
3504.028988	375132.005899	46.021402
3504.569572	375126.807561	46.026407
3504.498323	375135.569336	46.031412
3504.444318	375118.204150	46.036417
3504.181735	375103.059548	46.041421
3504.306809	375102.963503	46.046426
3504.360147	375099.393869	46.051431
3504.320072	375108.812095	46.056436
3504.193136	375098.606348	46.061441
3504.445899	375104.162668	46.066445
3504.175110	375114.685736	46.071450
3504.279895	375071.603613	46.076455
3504.482957	375100.163247	46.081460
3504.090233	375074.889666	46.086465
3504.520793	375097.766223	46.091469
3503.972326	375078.469626	46.096474
3504.499978	375079.632690	46.101479
3504.158768	375092.252767	46.106484
3504.800795	375066.942798	46.111489
3504.379522	375049.635639	46.116493
3504.265663	375064.356533	46.121498
3504.783913	375035.657491	46.126503
3504.502464	375045.317388	46.131508
3504.283121	375044.054788	46.136513
3504.558842	375002.853383	46.141517
3503.961054	375009.765169	46.146522
3504.461549	375011.746527	46.151527
3503.992721	375004.113115	46.156532
3504.369924	375013.312776	46.161537
3504.640611	375012.506900	46.166541
3504.260946	375012.185392	46.171546
3504.482433	374978.801847	46.176551
3504.513667	374974.065570	46.181556
3504.283899	374963.392732	46.186561
3504.246650	374984.282863	46.191565
3504.516704	374964.271759	46.196570
3504.334550	374962.112965	46.201575
3504.025652	374974.295532	46.206580
3504.156638	374948.226836	46.211585
3504.181946	374946.798372	46.216589
3504.093278	374939.104852	46.221594
3504.259373	374939.867199	46.226599
3504.096249	374946.684847	46.231604
3504.040095	374954.630273	46.236609
3504.034555	374928.735771	46.241613
3503.956414	374954.872516	46.246618
3504.090668	374949.687512	46.251623
3504.094103	374947.372192	46.256628
3504.318643	374934.567090	46.261633
3504.386737	374939.516686	46.266637
3504.435380	374953.143555	46.271642
3504.633674	374939.147040	46.276647
3504.415598	374926.513653	46.281652
3504.479153	374900.531899	46.286657
3504.517444	374900.856573	46.291661
3504.226894	374907.923308	46.296666
3504.753403	374900.107098	46.301671
3504.579527	374899.269745	46.306676
3504.008674	374870.412062	46.311681
3504.142949	374872.756570	46.316685
3503.973359	374886.850398	46.321690
3504.000993	374874.966719	46.326695
3504.088764	374891.690809	46.331700
3504.350007	374878.727262	46.336705
3504.302344	374888.299364	46.341709
3504.439175	374877.950116	46.346714
3504.420446	374856.916232	46.351719
3504.230082	374850.815902	46.356724
3504.315618	374838.159932	46.361729
3504.390696	374832.526391	46.366733
3503.943821	374834.479454	46.371738
3504.290923	374830.685295	46.376743
3504.116136	374837.530242	46.381748
3504.286710	374845.999476	46.386753
3504.190591	374843.292885	46.391757
3504.060647	374840.795142	46.396762
3504.378334	374834.309248	46.401767
3503.922099	374829.650012	46.406772
3504.207070	374816.021317	46.411777
3504.234176	374814.389063	46.416781
3503.928031	374819.881147	46.421786
3503.940125	374810.747168	46.426791
3504.094907	374819.829407	46.431796
3504.158875	374810.865291	46.436801
3504.436605	374806.318968	46.441805
3504.335121	374818.672295	46.446810
3504.400974	374814.413841	46.451815
3504.056542	374820.573355	46.456820
3504.179481	374821.189900	46.461825
3504.053356	374831.181420	46.466829
3504.021135	374829.329606	46.471834
3504.210280	374817.852819	46.476839
3503.938836	374807.313717	46.481844
3504.089646	374799.099000	46.486849
3504.101285	374793.806172	46.491853
3503.724545	374799.767295	46.496858
3503.955395	374794.414376	46.501863
3503.690759	374808.218004	46.506868
3503.955861	374822.802767	46.511873
3504.278456	374832.825104	46.516877
3504.190611	374818.212402	46.521882
3504.559882	374804.773878	46.526887
3504.189392	374800.635275	46.531892
3504.241597	374800.041995	46.536897
3504.337558	374804.987202	46.541901
3504.067674	374803.427333	46.546906
3504.731053	374796.174532	46.551911
3503.907081	374806.149184	46.556916
3503.932016	374805.916343	46.561921
3504.359383	374795.190458	46.566925
3504.087893	374792.282648	46.571930
3504.253322	374773.890560	46.576935
3504.096491	374771.804066	46.581940
3504.254173	374763.257566	46.586945
3504.279366	374772.716427	46.591949
3504.259264	374766.996173	46.596954
3504.428279	374760.813583	46.601959
3504.131578	374767.118185	46.606964
3504.283438	374772.436124	46.611969
3504.818203	374758.411796	46.616973
3504.073588	374743.928326	46.621978
3503.968931	374739.035439	46.626983
3503.939332	374738.251589	46.631988
3504.086015	374735.659236	46.636993
3504.241040	374737.440843	46.641997
3504.359890	374734.802014	46.647002
3504.315357	374735.852037	46.652007
3504.122784	374740.028856	46.657012
3504.141441	374737.965495	46.662017
3504.229493	374732.838643	46.667021
3504.133219	374744.860478	46.672026
3504.324212	374738.776161	46.677031
3504.176505	374713.412750	46.682036
3504.299601	374701.819183	46.687041
3504.269483	374696.151378	46.692045
3504.189012	374719.515932	46.697050
3504.328674	374708.657441	46.702055
3504.024744	374716.464017	46.707060
3504.281481	374708.436039	46.712065
3504.155907	374712.551395	46.717069
3504.104337	374721.742588	46.722074
3504.112241	374723.369388	46.727079
3504.167209	374719.850338	46.732084
3504.070035	374701.728670	46.737089
3503.994348	374685.078983	46.742093
3503.886609	374683.595228	46.747098
3504.392842	374663.648394	46.752103
3504.047706	374687.258306	46.757108
3503.895823	374675.784513	46.762113
3504.186287	374667.064377	46.767117
3504.605993	374671.729483	46.772122
3504.197177	374680.290340	46.777127
3504.118183	374693.225217	46.782132
3504.342999	374684.413711	46.787137
3504.330952	374689.172504	46.792141
3504.157635	374686.859672	46.797146
3504.167324	374673.808637	46.802151
3504.122391	374666.642345	46.807156
3504.080511	374663.672792	46.812161
3504.444055	374656.391051	46.817165
3504.064989	374650.752962	46.822170
3504.192684	374651.724886	46.827175
3504.072885	374652.761371	46.832180
3504.313201	374647.559564	46.837185
3504.244763	374656.473623	46.842189
3503.984105	374656.056987	46.847194
3504.205229	374657.879024	46.852199
3504.180956	374659.739853	46.857204
3504.339700	374662.818198	46.862209
3504.115904	374646.878727	46.867213
3503.836115	374632.601554	46.872218
3504.192030	374621.123787	46.877223
3504.103281	374626.785032	46.882228
3504.015154	374625.832368	46.887233
3504.015362	374629.037528	46.892237
3504.074786	374637.041058	46.897242
3504.243455	374635.793423	46.902247
3503.986629	374634.613049	46.907252
3503.908653	374627.731788	46.912257
3503.829380	374629.117996	46.917261
3503.935340	374620.172639	46.922266
3504.341095	374615.097302	46.927271
3503.888302	374632.949895	46.932276
3503.954643	374636.144601	46.937281
3504.036077	374630.331963	46.942285
3503.922559	374638.235643	46.947290
3504.037264	374633.053690	46.952295
3503.903256	374626.003223	46.957300
3503.787017	374638.028245	46.962305
3503.915902	374640.348181	46.967309
3503.848353	374653.586514	46.972314
3503.854460	374644.071879	46.977319
3504.111985	374646.193415	46.982324
3503.948114	374655.402375	46.987329
3504.395158	374640.069112	46.992333
3504.173688	374649.592432	46.997338
3504.184089	374648.064562	47.002343
3504.163428	374641.301432	47.007348
3504.301340	374641.915613	47.012353
3504.262701	374656.090571	47.017357
3503.805933	374651.609463	47.022362
3504.421353	374651.486779	47.027367
3504.075141	374660.342996	47.032372
3504.236107	374648.082047	47.037377
3504.433623	374647.236856	47.042381
3504.324075	374642.192104	47.047386
3504.345092	374637.813531	47.052391
3504.174472	374635.195017	47.057396
3504.151006	374632.680430	47.062401
3504.478360	374634.231298	47.067405
3504.579087	374626.914785	47.072410
3504.676401	374617.207662	47.077415
3504.391749	374609.036306	47.082420
3504.343135	374591.695483	47.087425
3504.231913	374591.077159	47.092429
3504.274267	374590.917876	47.097434
3504.496510	374586.634677	47.102439
3504.406543	374587.208568	47.107444
3504.288052	374561.687819	47.112449
3504.408298	374553.783138	47.117453
3504.280247	374554.719179	47.122458
3504.288339	374569.293783	47.127463
3504.110819	374565.786034	47.132468
3504.263751	374558.766509	47.137473
3504.300130	374564.509734	47.142477
3503.993520	374558.732990	47.147482
3504.310632	374561.938936	47.152487
3504.311972	374553.976738	47.157492
3504.363876	374534.305163	47.162497
3504.529568	374519.296147	47.167501
3504.095109	374531.422380	47.172506
3504.487931	374530.190183	47.177511
3504.127974	374534.037354	47.182516
3504.086974	374534.145625	47.187521
3504.233626	374522.777224	47.192525
3504.036977	374524.309179	47.197530
3504.373099	374517.616818	47.202535
3504.223726	374517.462404	47.207540
3504.049426	374501.515053	47.212545
3504.249879	374501.890409	47.217549
3503.634200	374523.940599	47.222554
3504.222278	374497.188854	47.227559
3504.218848	374507.797002	47.232564
3503.954073	374506.058249	47.237569
3504.368822	374499.328018	47.242573
3503.863122	374503.452609	47.247578
3504.188033	374501.773266	47.252583
3504.257934	374507.765578	47.257588
3504.293076	374511.601171	47.262593
3504.332290	374510.526622	47.267597
3504.190656	374496.125811	47.272602
3504.176218	374475.523496	47.277607
3504.250345	374481.413392	47.282612
3504.000725	374474.355736	47.287617
3504.534221	374463.511238	47.292621
3504.238259	374490.751099	47.297626
3504.425662	374467.420464	47.302631
3504.247317	374473.986218	47.307636
3504.058360	374474.575759	47.312641
3504.186874	374483.128030	47.317645
3503.918865	374482.509051	47.322650
3504.175256	374465.552403	47.327655
3504.312729	374461.791348	47.332660
3504.063333	374456.285362	47.337665
3504.080958	374434.991136	47.342669
3504.117326	374436.969578	47.347674
3504.342932	374459.726263	47.352679
3504.339041	374436.374974	47.357684
3504.073501	374448.398216	47.362689
3504.191848	374449.040931	47.367693
3503.921708	374440.307615	47.372698
3504.067206	374460.304237	47.377703
3504.068235	374451.553495	47.382708
3503.982188	374450.600498	47.387713
3504.186647	374462.549439	47.392717
3504.187443	374442.809586	47.397722
3504.345264	374449.805522	47.402727
3504.416416	374460.834336	47.407732
3504.428217	374423.159054	47.412737
3504.452667	374398.455057	47.417741
3504.196403	374439.272501	47.422746
3504.279986	374413.821468	47.427751
3504.103681	374410.364388	47.432756
3504.031740	374420.805324	47.437761
3504.180617	374404.806848	47.442765
3504.090719	374421.660965	47.447770
3504.260931	374429.418082	47.452775
3504.377440	374398.187440	47.457780
3503.929996	374378.950857	47.462785
3504.255685	374380.501998	47.467789
3504.008703	374394.023158	47.472794
3504.185137	374379.750091	47.477799
3504.350346	374389.415848	47.482804
3504.187091	374393.282813	47.487809
3504.115215	374392.912646	47.492813
3504.060878	374397.474654	47.497818
3504.301340	374390.161447	47.502823
3504.124372	374397.159440	47.507828
3504.036804	374380.867638	47.512833
3504.323941	374416.257249	47.517837
3503.834166	374392.473985	47.522842
3504.359174	374401.421478	47.527847
3504.475576	374379.806355	47.532852
3504.057726	374363.617632	47.537857
3503.967225	374353.660320	47.542861
3503.813327	374359.102960	47.547866
3504.166040	374354.366668	47.552871
3504.148998	374359.762236	47.557876
3503.877087	374352.453704	47.562881
3504.068996	374356.951352	47.567885
3503.778799	374369.156580	47.572890
3504.071009	374335.735896	47.577895
3504.082346	374366.819263	47.582900
3503.865601	374359.730952	47.587905
3504.114103	374351.577017	47.592909
3503.764295	374358.322521	47.597914
3504.428584	374359.769262	47.602919
3503.979873	374360.094611	47.607924
3504.051638	374371.454045	47.612929
3504.029078	374351.183644	47.617933
3504.080625	374382.464146	47.622938
3503.925002	374353.972905	47.627943
3504.041457	374375.754812	47.632948
3504.278292	374343.691096	47.637953
3504.074069	374384.424054	47.642957
3504.068983	374349.651293	47.647962
3504.049667	374389.998885	47.652967
3504.291896	374365.514821	47.657972
3504.164759	374377.668832	47.662977
3504.413499	374357.813430	47.667981
3503.911751	374343.978249	47.672986
3504.281274	374346.539979	47.677991
3504.182485	374325.823733	47.682996
3503.958610	374345.293729	47.688001
3503.977485	374351.090626	47.693005
3504.076083	374338.178059	47.698010
3503.911884	374346.624002	47.703015
3504.273647	374333.847898	47.708020
3504.156240	374338.190941	47.713025
3504.309401	374334.605460	47.718029
3504.350078	374342.026939	47.723034
3504.413695	374336.115326	47.728039
3504.423026	374343.770701	47.733044
3504.237781	374324.874213	47.738049
3504.254920	374298.645037	47.743053
3503.742322	374315.744083	47.748058
3504.456357	374308.610379	47.753063
3504.250072	374313.399920	47.758068
3504.166123	374301.075832	47.763073
3504.371815	374315.568414	47.768077
3504.164585	374314.227563	47.773082
3504.353747	374319.107219	47.778087
3504.292272	374315.581104	47.783092
3504.036193	374303.818423	47.788097
3504.336447	374274.593676	47.793101
3504.317037	374289.249041	47.798106
3504.373826	374281.710471	47.803111
3504.624762	374281.212959	47.808116
3504.365257	374282.831172	47.813121
3504.484817	374281.006217	47.818125
3504.008964	374249.360343	47.823130
3504.293134	374247.026043	47.828135
3504.202320	374255.816536	47.833140
3504.184486	374232.798029	47.838145
3503.940592	374247.310829	47.843149
3504.005105	374258.315309	47.848154
3503.943829	374227.392460	47.853159
3503.953454	374271.780231	47.858164
3503.885892	374245.971418	47.863169
3503.881348	374256.376304	47.868173
3504.105996	374220.091716	47.873178
3503.950247	374259.214541	47.878183
3503.953356	374244.790761	47.883188
3504.038922	374249.101728	47.888193
3504.375287	374221.244886	47.893197
3504.061573	374273.493229	47.898202
3504.234303	374233.324853	47.903207
3504.046337	374268.331810	47.908212
3504.139118	374245.957212	47.913217
3504.321237	374262.768395	47.918221
3504.357436	374262.482893	47.923226
3504.307680	374241.199219	47.928231
3503.907229	374231.418063	47.933236
3504.010770	374239.999770	47.938241
3504.413380	374201.880938	47.943245
3504.054068	374223.025871	47.948250
3504.470343	374203.271101	47.953255
3504.223906	374222.897348	47.958260
3504.235843	374231.646166	47.963265
3504.594704	374214.444275	47.968269
3504.419645	374222.332324	47.973274
3504.314568	374196.020650	47.978279
3504.164715	374170.758996	47.983284
3504.344482	374188.613540	47.988289
3504.306994	374196.632475	47.993293
3503.853555	374170.096035	47.998298
3504.260455	374192.900523	48.003303
3504.093185	374186.465750	48.008308
3504.385432	374180.085526	48.013313
3504.199452	374200.109236	48.018317
3503.968818	374198.314197	48.023322
3504.104390	374200.582224	48.028327
3504.151899	374170.557904	48.033332
3503.968313	374204.597578	48.038337
3504.173939	374155.546064	48.043341
3503.920402	374174.588382	48.048346
3503.905662	374170.825925	48.053351
3504.293452	374151.380889	48.058356
3503.924343	374166.574900	48.063361
3504.087727	374180.896151	48.068365
3503.928410	374149.810676	48.073370
3504.203042	374175.790397	48.078375
3504.030284	374188.384122	48.083380
3504.004568	374159.032756	48.088385
3504.155223	374181.928633	48.093389
3504.119872	374180.407979	48.098394
3503.943678	374186.235736	48.103399
3504.251617	374143.476660	48.108404
3504.198404	374187.925331	48.113409
3504.020888	374183.781598	48.118413
3503.926281	374170.594263	48.123418
3504.679084	374143.790812	48.128423
3504.153365	374192.740388	48.133428
3504.126351	374185.520303	48.138433
3504.661924	374139.392860	48.143437
3504.002126	374152.674099	48.148442
3503.923918	374165.049380	48.153447
3504.436282	374118.798392	48.158452
3504.207909	374150.123320	48.163457
3504.127877	374147.617644	48.168461
3504.391646	374115.702122	48.173466
3504.248898	374159.071141	48.178471
3503.912839	374161.998800	48.183476
3504.413208	374132.030054	48.188481
3504.432573	374155.989659	48.193485
3504.250198	374116.360626	48.198490
3504.366089	374135.217373	48.203495
3504.232143	374095.936798	48.208500
3504.122609	374121.748339	48.213505
3504.190843	374122.704237	48.218509
3504.205701	374096.780549	48.223514
3504.520300	374091.821310	48.228519
3504.419890	374138.465169	48.233524
3504.104917	374112.593630	48.238529
3504.500795	374056.948907	48.243533
3504.272041	374098.932490	48.248538
3504.045855	374065.822477	48.253543
3504.508916	374078.519231	48.258548
3504.206474	374071.469856	48.263553
3504.613574	374061.204870	48.268557
3504.081088	374087.642930	48.273562
3504.114945	374048.055964	48.278567
3504.216966	374027.435015	48.283572
3504.176188	374056.822500	48.288577
3504.727272	374018.069515	48.293581
3504.242847	374058.643582	48.298586
3504.338123	374025.559035	48.303591
3504.227421	374051.879567	48.308596
3504.328660	374036.855126	48.313601
3504.231602	374038.091536	48.318605
3504.100831	374018.575782	48.323610
3504.280971	373991.125053	48.328615
3504.130687	374020.707941	48.333620
3504.272018	373997.867648	48.338625
3504.119438	374002.572421	48.343629
3503.945570	374006.135842	48.348634
3504.004394	373992.364558	48.353639
3503.974252	374026.430999	48.358644
3504.269393	373998.020885	48.363649
3503.842366	374019.685388	48.368653
3503.655933	374001.959093	48.373658
3504.066226	374016.470314	48.378663
3504.202853	374017.771536	48.383668
3504.097321	374011.683110	48.388673
3504.471212	374020.858079	48.393677
3503.702341	374023.599784	48.398682
3503.990296	374000.405619	48.403687
3504.203768	374037.765935	48.408692
3503.984790	374001.296901	48.413697
3504.241430	374031.222466	48.418701
3503.846234	374013.478301	48.423706
3504.169788	374035.278527	48.428711
3503.775745	374019.569230	48.433716
3503.525381	374017.421168	48.438721
3503.963000	374025.186966	48.443725
3504.125952	374028.188380	48.448730
3504.093805	374022.444488	48.453735
3504.289227	374026.661798	48.458740
3503.894275	374031.862767	48.463745
3504.192658	374028.788504	48.468749
3503.806615	374038.134474	48.473754
3504.212478	374025.961818	48.478759
3504.074970	374025.474831	48.483764
3503.904257	374021.737016	48.488769
3504.085969	374025.931056	48.493773
3503.604111	374038.675440	48.498778
3503.846374	374016.658660	48.503783
3503.936654	374036.511587	48.508788
3503.965655	374043.349890	48.513793
3504.303147	374032.688891	48.518797
3504.087562	374045.899944	48.523802
3504.149231	374034.748347	48.528807
3504.097467	374020.918239	48.533812
3503.974994	374032.308471	48.538817
3504.484917	374023.782452	48.543821
3503.929850	374015.119524	48.548826
3503.852499	374004.142524	48.553831
3503.864860	374005.946715	48.558836
3504.084428	374006.344493	48.563841
3504.389122	373996.858823	48.568845
3503.954875	374009.926386	48.573850
3503.881869	374015.051026	48.578855
3503.913347	374011.204933	48.583860
3503.600891	374006.726380	48.588865
3504.139309	374026.228652	48.593869
3504.127897	374008.601884	48.598874
3504.379090	374003.932477	48.603879
3503.959116	374017.430229	48.608884
3503.865975	374020.294059	48.613889
3504.543739	374002.583783	48.618893
3504.034222	374008.082684	48.623898
3504.308688	374014.780436	48.628903
3504.397072	374009.780633	48.633908
3504.395207	374009.195889	48.638913
3504.452790	373994.152896	48.643917
3504.313879	373980.667246	48.648922
3504.388892	373977.653727	48.653927
3504.005756	373979.444124	48.658932
3503.695661	373980.841403	48.663937
3504.231283	373973.074455	48.668941
3504.019768	373978.856948	48.673946
3504.072170	373984.267025	48.678951
3504.215353	373990.756591	48.683956
3504.138961	373989.038913	48.688961
3504.367094	373978.980264	48.693965
3504.430001	373980.445771	48.698970
3504.286747	373975.431704	48.703975
3504.243349	373948.296101	48.708980
3504.014746	373943.422713	48.713985
3504.310563	373965.659809	48.718989
3504.081594	373944.327997	48.723994
3504.134918	373954.011542	48.728999
3504.555077	373946.644413	48.734004
3504.365959	373960.080252	48.739009
3504.366572	373951.329471	48.744013
3504.160215	373946.147309	48.749018
3504.144519	373938.162247	48.754023
3504.008896	373928.517223	48.759028
3503.966909	373929.490549	48.764033
3504.445706	373901.331156	48.769037
3504.074351	373911.107282	48.774042
3504.062795	373920.165137	48.779047
3504.420733	373898.689648	48.784052
3504.205174	373915.640151	48.789057
3504.439718	373912.881229	48.794061
3504.389664	373905.283164	48.799066
3504.051957	373922.049468	48.804071
3504.364681	373885.903293	48.809076
3504.062219	373879.515281	48.814081
3503.946152	373890.650158	48.819085
3504.008820	373884.916697	48.824090
3504.044511	373894.221471	48.829095
3504.076675	373892.486628	48.834100
3504.090440	373887.752988	48.839105
3504.345489	373889.213562	48.844109
3504.181102	373898.575401	48.849114
3504.545608	373872.189290	48.854119
3503.960512	373880.040470	48.859124
3504.059901	373893.023713	48.864129
3504.324372	373877.057636	48.869133
3504.285927	373886.526760	48.874138
3503.983667	373874.160740	48.879143
3504.245613	373865.801079	48.884148
3504.044191	373858.812013	48.889153
3504.353430	373848.740512	48.894157
3504.009465	373860.496501	48.899162
3504.377160	373843.140430	48.904167
3504.406690	373856.109290	48.909172
3504.144738	373852.614826	48.914177
3504.545400	373855.883935	48.919181
3504.074050	373864.047833	48.924186
3504.065869	373845.937159	48.929191
3503.991421	373858.286499	48.934196
3504.313081	373860.270747	48.939201
3504.254056	373820.265796	48.944205
3504.102841	373830.465030	48.949210
3504.224915	373811.596042	48.954215
3504.408860	373796.024237	48.959220
3503.809313	373835.853573	48.964225
3504.514301	373789.495454	48.969229
3504.058251	373826.147773	48.974234
3504.419927	373824.844166	48.979239
3504.354917	373803.359171	48.984244
3504.297403	373829.747751	48.989249
3503.900909	373787.506674	48.994253
3504.048665	373797.149890	48.999258
3503.924288	373768.576992	49.004263
3503.931947	373791.368498	49.009268
3503.962823	373777.092795	49.014273
3503.982794	373788.791274	49.019277
3503.945674	373785.541084	49.024282
3504.057288	373774.330646	49.029287
3503.934499	373793.759482	49.034292
3503.877981	373787.765028	49.039297
3504.279201	373783.885905	49.044301
3504.139681	373791.488597	49.049306
3504.137020	373795.889874	49.054311
3504.176786	373788.938984	49.059316
3503.768082	373790.402733	49.064321
3504.050276	373779.089017	49.069325
3504.114904	373801.260994	49.074330
3504.018064	373791.457177	49.079335
3504.102710	373796.531485	49.084340
3504.076315	373799.715476	49.089345
3504.149814	373793.954853	49.094349
3504.006200	373790.746936	49.099354
3503.633823	373804.593368	49.104359
3504.227124	373783.156929	49.109364
3504.061369	373779.469184	49.114369
3504.356014	373808.524002	49.119373
3504.613331	373795.204601	49.124378
3504.141192	373790.700390	49.129383
3504.328251	373799.396177	49.134388
3504.034554	373771.536879	49.139393
3504.057182	373756.524763	49.144397
3503.747528	373773.006871	49.149402
3504.185559	373753.680898	49.154407
3504.244625	373752.145303	49.159412
3504.076961	373783.486349	49.164417
3504.332962	373767.750514	49.169421
3504.630374	373765.515847	49.174426
3504.324465	373764.979163	49.179431
3504.258620	373774.376329	49.184436
3503.954039	373757.965958	49.189441
3504.008822	373776.781652	49.194445
3504.054678	373775.095517	49.199450
3504.033524	373758.996478	49.204455
3504.301879	373785.664270	49.209460
3504.169501	373732.035923	49.214465
3504.397787	373748.840017	49.219469
3503.992145	373717.309828	49.224474
3504.015694	373742.490049	49.229479
3504.033823	373720.432227	49.234484
3503.979163	373753.841372	49.239489
3503.987398	373717.158103	49.244493
3503.611635	373760.081047	49.249498
3503.927690	373725.816638	49.254503
3504.067083	373737.419939	49.259508
3503.531421	373744.729125	49.264513
3504.003860	373741.322067	49.269517
3503.890878	373737.702291	49.274522
3504.265627	373758.807736	49.279527
3504.181087	373739.818747	49.284532
3503.923129	373733.423677	49.289537
3504.215453	373738.897613	49.294541
3504.079842	373749.399660	49.299546
3503.830779	373744.020716	49.304551
3503.977743	373741.631763	49.309556
3503.660885	373744.454663	49.314561
3504.099264	373747.285367	49.319565
3504.238983	373748.942245	49.324570
3504.149185	373749.261738	49.329575
3504.316876	373741.934482	49.334580
3504.077758	373761.814174	49.339585
3504.418027	373743.165045	49.344589
3504.499254	373741.447879	49.349594
3504.685526	373739.993928	49.354599
3504.492081	373737.302650	49.359604
3504.516702	373725.571746	49.364609
3504.337651	373716.823878	49.369613
3504.441508	373717.367142	49.374618
3504.420794	373730.216792	49.379623
3504.226847	373686.697118	49.384628
3503.787084	373696.153410	49.389633
3504.124540	373683.024812	49.394637
3503.847509	373683.475656	49.399642
3504.052491	373685.809055	49.404647
3504.141323	373678.239871	49.409652
3504.153737	373676.813401	49.414657
3504.090289	373691.399624	49.419661
3504.060709	373684.917569	49.424666
3504.190830	373661.417467	49.429671
3503.976057	373691.672181	49.434676
3504.382129	373686.113353	49.439681
3504.206708	373676.907012	49.444685
3503.855865	373695.303536	49.449690
3503.868807	373675.434205	49.454695
3504.247635	373696.030271	49.459700
3504.187719	373685.101307	49.464705
3504.280232	373685.188474	49.469709
3504.103995	373689.820707	49.474714
3503.880748	373690.695500	49.479719
3503.865713	373699.982898	49.484724
3503.926053	373693.995396	49.489729
3504.117468	373694.830078	49.494733
3504.068648	373692.294003	49.499738
3504.033466	373698.710057	49.504743
3503.852825	373708.125385	49.509748
3504.358025	373693.520290	49.514753
3504.089255	373675.781433	49.519757
3503.731805	373680.874764	49.524762
3504.151260	373671.421755	49.529767
3504.079155	373659.426302	49.534772
3503.729753	373668.079728	49.539777
3504.059232	373672.708335	49.544781
3503.986782	373673.839112	49.549786
3503.990796	373653.004526	49.554791
3503.944053	373670.004757	49.559796
3503.822277	373673.407343	49.564801
3504.019689	373684.060269	49.569805
3503.717289	373697.743045	49.574810
3503.671677	373723.112279	49.579815
3504.094180	373702.109809	49.584820
3503.485434	373711.770879	49.589825
3504.153726	373710.927564	49.594829
3504.077528	373704.503758	49.599834
3504.132596	373714.695850	49.604839
3504.203544	373709.647890	49.609844
3504.099010	373698.268093	49.614849
3504.291277	373712.305120	49.619853
3503.960011	373704.191830	49.624858
3503.990493	373677.909274	49.629863
3504.071746	373677.413140	49.634868
3503.828142	373704.721557	49.639873
3504.149226	373683.633357	49.644877
3503.978581	373696.176020	49.649882
3504.015413	373679.177443	49.654887
3503.774295	373697.047855	49.659892
3504.314076	373675.416314	49.664897
3504.200800	373695.555966	49.669901
3504.096738	373663.927186	49.674906
3503.802930	373692.947915	49.679911
3503.898565	373649.865754	49.684916
3503.720874	373699.549485	49.689921
3504.134855	373659.952936	49.694925
3504.079775	373688.325410	49.699930
3504.336686	373662.388626	49.704935
3504.293716	373693.837219	49.709940
3504.209322	373672.736796	49.714945
3504.141534	373695.158707	49.719949
3504.036575	373674.341357	49.724954
3504.061287	373697.130219	49.729959
3504.414260	373685.067577	49.734964
3503.965832	373677.405254	49.739969
3504.192119	373694.718452	49.744973
3504.306116	373693.759253	49.749978
3504.190930	373663.862037	49.754983
3504.186743	373667.424103	49.759988
3504.141939	373641.789384	49.764993
3504.055866	373645.288081	49.769997
3504.098848	373651.106704	49.775002
3504.235660	373660.319231	49.780007
3504.436900	373648.789331	49.785012
3504.120038	373654.766591	49.790017
3504.002099	373645.423965	49.795021
3504.179904	373665.619371	49.800026
3504.228165	373635.085777	49.805031
3503.662905	373658.883702	49.810036
3503.498706	373664.811390	49.815041
3504.009902	373660.024528	49.820045
3504.218803	373638.775971	49.825050
3504.268076	373655.226826	49.830055
3504.205733	373646.714877	49.835060
3504.042408	373645.646885	49.840065
3504.357546	373666.965307	49.845069
3504.395645	373646.786725	49.850074
3504.394959	373638.112398	49.855079
3504.271701	373636.198606	49.860084
3504.136861	373634.820851	49.865089
3504.238710	373623.281217	49.870093
3504.013918	373618.305435	49.875098
3504.056403	373634.960877	49.880103
3504.469632	373617.928213	49.885108
3503.928067	373635.439132	49.890113
3504.129369	373624.443420	49.895117
3504.109914	373624.675480	49.900122
3503.934038	373635.692687	49.905127
3504.095337	373634.268119	49.910132
3504.251624	373633.505740	49.915137
3504.266641	373606.080858	49.920141
3504.407321	373605.651644	49.925146
3504.193135	373580.196292	49.930151
3504.248937	373603.768881	49.935156
3504.292492	373580.994692	49.940161
3504.380022	373582.329128	49.945165
3504.231872	373567.089556	49.950170
3504.233048	373611.046918	49.955175
3504.239839	373590.415368	49.960180
3504.361207	373578.287554	49.965185
3504.326929	373548.046766	49.970189
3504.151533	373567.789285	49.975194
3503.954881	373561.766073	49.980199
3504.393405	373551.775817	49.985204
3503.914821	373559.559343	49.990209
3504.053397	373546.563894	49.995213
3503.824841	373572.496345	50.000218
3504.268451	373552.279053	50.005223
3504.121062	373581.887235	50.010228
3504.153287	373545.403530	50.015233
3504.247146	373573.065702	50.020237
3504.423670	373554.874826	50.025242
3504.085615	373563.348411	50.030247
3504.485887	373515.537291	50.035252
3504.134806	373529.253256	50.040257
3504.055460	373512.476483	50.045261
3504.088383	373539.207089	50.050266
3504.301782	373528.158564	50.055271
3504.355631	373522.553639	50.060276
3503.583370	373538.625638	50.065281
3504.108416	373524.195415	50.070285
3504.124905	373514.704318	50.075290
3504.347623	373544.355774	50.080295
3504.353516	373518.153320	50.085300
3504.189554	373534.434423	50.090305
3504.024755	373534.969281	50.095309
3503.775011	373490.924016	50.100314
3503.868464	373536.215107	50.105319
3504.251218	373521.247732	50.110324
3503.916914	373528.448811	50.115329
3503.936804	373523.256269	50.120333
3504.176471	373539.829703	50.125338
3503.575747	373537.965945	50.130343
3504.262523	373517.939144	50.135348
3503.891354	373527.435508	50.140353
3503.832805	373535.228955	50.145357
3503.727378	373534.024616	50.150362
3503.730181	373526.367250	50.155367
3504.062049	373559.511942	50.160372
3503.879947	373540.894421	50.165377
3504.074696	373546.129423	50.170381
3504.207572	373556.894337	50.175386
3504.365094	373539.138911	50.180391
3504.267948	373532.947335	50.185396
3503.996882	373531.921810	50.190401
3504.499040	373494.829567	50.195405
3503.807562	373520.199268	50.200410
3503.871432	373516.424325	50.205415
3504.312808	373513.454611	50.210420
3503.949194	373517.175262	50.215425
3504.001897	373519.609057	50.220429
3504.213096	373528.275647	50.225434
3504.050380	373519.983046	50.230439
3503.986039	373522.689728	50.235444
3503.989530	373522.180446	50.240449
3504.228038	373515.935808	50.245453
3504.042872	373525.275578	50.250458
3504.270060	373517.277479	50.255463
3504.591350	373503.439104	50.260468
3503.700498	373539.142871	50.265473
3504.459588	373522.971278	50.270477
3504.269809	373502.752334	50.275482
3504.265160	373489.372493	50.280487
3504.386943	373466.534998	50.285492
3504.008887	373497.807763	50.290497
3504.360751	373487.424176	50.295501
3504.180286	373473.258093	50.300506
3503.861894	373490.377655	50.305511
3504.297192	373452.507352	50.310516
3504.000287	373495.672488	50.315521
3504.213271	373473.278471	50.320525
3504.205936	373480.351556	50.325530
3504.134899	373492.573274	50.330535
3504.053893	373466.969608	50.335540
3503.791933	373492.474936	50.340545
3504.177013	373469.570382	50.345549
3504.284012	373470.392976	50.350554
3504.099502	373464.876599	50.355559
3504.223708	373464.831565	50.360564
3504.384370	373442.318611	50.365569
3503.875917	373445.578833	50.370573
3504.266996	373429.338185	50.375578
3504.062426	373464.297569	50.380583
3504.325724	373446.957836	50.385588
3504.074342	373450.762504	50.390593
3504.372363	373463.358344	50.395597
3504.236492	373445.267680	50.400602
3504.118801	373458.234498	50.405607
3504.596052	373446.279334	50.410612
3504.241529	373412.909264	50.415617
3504.085968	373404.488316	50.420621
3503.906327	373413.649168	50.425626
3504.146233	373398.984154	50.430631
3503.783915	373427.837827	50.435636
3504.011010	373396.665265	50.440641
3503.674290	373410.048299	50.445645
3503.873421	373422.507153	50.450650
3504.052421	373401.822848	50.455655
3504.265102	373423.997061	50.460660
3503.960294	373412.343583	50.465665
3503.993841	373412.923404	50.470669
3504.148920	373430.375161	50.475674
3504.066906	373428.353086	50.480679
3504.094050	373412.169962	50.485684
3503.942237	373419.494843	50.490689
3503.921047	373420.464893	50.495693
3504.048939	373413.576326	50.500698
3503.823396	373425.491787	50.505703
3504.288285	373413.360498	50.510708
3504.064164	373404.848635	50.515713
3503.717364	373431.613897	50.520717
3504.147222	373424.041635	50.525722
3504.187282	373417.904668	50.530727
3504.135728	373410.688328	50.535732
3503.940646	373387.163162	50.540737
3503.864665	373361.507760	50.545741
3503.956095	373326.057482	50.550746
3503.576785	373265.344778	50.555751
3503.823227	373234.474299	50.560756
3503.470225	373134.530921	50.565761
3503.165780	373107.207088	50.570765
3503.027617	372987.361791	50.575770
3502.756704	372923.095469	50.580775
3502.117177	372794.781444	50.585780
3501.686258	372727.207624	50.590785
3501.948278	372604.677764	50.595789
3501.479541	372504.929250	50.600794
3500.900861	372395.963487	50.605799
3500.917399	372269.197686	50.610804
3500.210873	372135.295618	50.615809
3500.113602	372005.799576	50.620813
3499.525213	371872.488542	50.625818
3499.129407	371731.565675	50.630823
3498.839535	371570.019523	50.635828
3498.348851	371446.206111	50.640833
3498.139209	371280.931984	50.645837
3497.761415	371122.806960	50.650842
3496.733068	370956.719721	50.655847
3496.827814	370787.070767	50.660852
3496.231605	370622.160478	50.665857
3495.708384	370440.549202	50.670861
3495.137534	370273.140416	50.675866
3494.533236	370099.706873	50.680871
3494.361145	369911.575975	50.685876
3493.499403	369726.860569	50.690881
3492.718778	369529.512913	50.695885
3492.313323	369364.186041	50.700890
3491.625061	369162.369955	50.705895
3491.224212	368968.648661	50.710900
3490.704595	368774.054837	50.715905
3490.028974	368595.945368	50.720909
3489.761478	368399.910749	50.725914
3488.956526	368176.457862	50.730919
3488.118910	367990.535531	50.735924
3487.428091	367787.594077	50.740929
3487.234642	367587.117256	50.745933
3486.700796	367392.061612	50.750938
3485.762844	367179.259478	50.755943
3485.291306	366978.645775	50.760948
3484.690855	366772.377892	50.765953
3484.072196	366557.792230	50.770957
3483.129743	366363.814381	50.775962
3482.547662	366156.192295	50.780967
3482.269592	365951.014590	50.785972
3481.225559	365745.906155	50.790977
3481.125770	365523.244432	50.795981
3480.256666	365305.740994	50.800986
3479.739313	365095.203270	50.805991
3478.953071	364896.436517	50.810996
3478.372838	364672.192752	50.816001
3477.373672	364453.967943	50.821005
3476.577489	364265.250279	50.826010
3476.187550	364041.863878	50.831015
3475.739761	363826.754858	50.836020
3474.575947	363630.612158	50.841025
3474.263457	363397.617946	50.846029
3473.626264	363182.230540	50.851034
3472.755177	362983.570718	50.856039
3472.097294	362759.228155	50.861044
3471.407343	362556.390401	50.866049
3470.698204	362335.387171	50.871053
3470.004011	362144.660062	50.876058
3469.496090	361907.312778	50.881063
3469.083400	361731.043195	50.886068
3468.005941	361486.684628	50.891073
3467.642961	361283.611585	50.896077
3467.156699	361053.152308	50.901082
3466.449826	360849.546533	50.906087
3466.047022	360623.041508	50.911092
3465.052787	360412.634387	50.916097
3464.758684	360175.142878	50.921101
3463.534148	359977.315148	50.926106
3462.838376	359727.950703	50.931111
3462.585943	359536.939760	50.936116
3461.318628	359310.107207	50.941121
3460.671188	359101.548035	50.946125
3460.611482	358895.694188	50.951130
3459.478104	358656.190409	50.956135
3459.006350	358457.983017	50.961140
3458.446826	358228.361618	50.966145
3457.688733	358024.344931	50.971149
3457.021100	357792.244773	50.976154
3456.174102	357581.853053	50.981159
3455.884046	357344.576185	50.986164
3455.100428	357163.513626	50.991169
3454.358068	356902.309084	50.996173
3453.406597	356721.118774	51.001178
3452.429904	356471.705924	51.006183
3451.865858	356286.152093	51.011188
3451.227073	356061.419269	51.016193
3450.801194	355846.042193	51.021197
3450.489825	355639.196747	51.026202
3449.615264	355433.482889	51.031207
3448.635889	355203.303251	51.036212
3448.153437	354994.929879	51.041217
3447.253503	354794.307196	51.046221
3446.604445	354568.805958	51.051226
3446.000069	354344.263732	51.056231
3445.411692	354145.243451	51.061236
3444.537180	353926.290025	51.066241
3443.950551	353713.296197	51.071245
3443.401379	353507.166918	51.076250
3442.652690	353287.172938	51.081255
3442.332588	353091.083811	51.086260
3441.129733	352865.179209	51.091265
3440.395011	352635.382150	51.096269
3439.776616	352444.733143	51.101274
3439.140900	352246.323935	51.106279
3438.520940	352000.116165	51.111284
3437.738577	351838.122300	51.116289
3437.349246	351591.392626	51.121293
3436.776339	351399.867379	51.126298
3435.749961	351168.023172	51.131303
3435.133814	350976.528705	51.136308
3434.715740	350753.214297	51.141313
3433.975484	350533.131263	51.146317
3433.149970	350339.580680	51.151322
3432.460351	350125.290799	51.156327
3431.858523	349902.052854	51.161332
3430.953247	349696.499674	51.166337
3430.568916	349500.178539	51.171341
3429.910841	349280.942820	51.176346
3428.850289	349060.039164	51.181351
3428.565906	348867.212286	51.186356
3427.601849	348654.410819	51.191361
3426.852873	348453.282356	51.196365
3426.381821	348232.205854	51.201370
3425.532774	348034.095030	51.206375
3424.994479	347819.823214	51.211380
3424.159577	347636.190983	51.216385
3423.678655	347406.789945	51.221389
3423.098877	347208.786365	51.226394
3422.316004	347004.909242	51.231399
3421.969224	346788.897937	51.236404
3421.253759	346583.023352	51.241409
3420.407189	346376.812420	51.246413
3419.835793	346154.801949	51.251418
3419.044679	345951.482348	51.256423
3418.648217	345735.831287	51.261428
3417.473623	345535.497957	51.266433
3416.624996	345321.113147	51.271437
3416.336895	345124.532574	51.276442
3415.660170	344924.245692	51.281447
3415.020672	344712.269110	51.286452
3414.526660	344503.399547	51.291457
3413.902453	344285.895599	51.296461
3413.253945	344087.586800	51.301466
3412.282717	343872.630672	51.306471
3411.671413	343657.005966	51.311476
3410.858182	343461.470152	51.316481
3410.354755	343244.859654	51.321485
3410.018035	343041.381820	51.326490
3409.157654	342829.153477	51.331495
3408.616742	342618.350229	51.336500
3407.887060	342415.263333	51.341505
3407.089637	342198.339219	51.346509
3406.385341	341989.545082	51.351514
3405.298703	341789.618012	51.356519
3405.147781	341576.025854	51.361524
3403.933697	341388.514106	51.366529
3403.633132	341172.475096	51.371533
3403.123068	340967.235935	51.376538
3402.327826	340755.244679	51.381543
3401.717990	340550.707213	51.386548
3400.675381	340348.986680	51.391553
3400.235952	340126.780383	51.396557
3399.797727	339922.901035	51.401562
3398.869934	339721.643996	51.406567
3398.789951	339502.586068	51.411572
3397.351760	339303.419405	51.416577
3396.770080	339101.596564	51.421581
3396.309650	338887.942401	51.426586
3395.363268	338675.229871	51.431591
3394.555666	338475.757283	51.436596
3393.907381	338285.473994	51.441601
3393.458931	338086.427084	51.446605
3392.905344	337885.512428	51.451610
3391.903169	337683.089796	51.456615
3391.477949	337477.189606	51.461620
3390.744950	337272.381156	51.466625
3390.224976	337070.924109	51.471629
3389.470539	336869.019848	51.476634
3388.616310	336657.788137	51.481639
3387.857007	336456.978036	51.486644
3387.334987	336267.458119	51.491649
3386.862481	336062.095618	51.496653
3385.691166	335865.472923	51.501658
3385.290707	335669.313276	51.506663
3384.812435	335460.742265	51.511668
3383.565922	335272.326951	51.516673
3383.269963	335070.192057	51.521677
3382.832505	334864.005757	51.526682
3382.229547	334677.549091	51.531687
3381.285584	334467.648536	51.536692
3381.018695	334266.805020	51.541697
3380.253771	334067.668971	51.546701
3380.010338	333855.211851	51.551706
3378.796126	333655.076444	51.556711
3378.441524	333437.951395	51.561716
3377.647928	333232.554858	51.566721
3376.762939	333041.632355	51.571725
3376.241799	332833.238440	51.576730
3375.499878	332618.183317	51.581735
3375.152720	332421.904254	51.586740
3374.407216	332218.584764	51.591745
3373.596190	332012.576468	51.596749
3372.874801	331808.615547	51.601754
3371.911066	331614.315715	51.606759
3371.597508	331395.472255	51.611764
3370.793597	331201.375175	51.616769
3370.147674	331005.215896	51.621773
3369.469746	330802.161806	51.626778
3368.771915	330603.463780	51.631783
3368.194793	330391.201952	51.636788
3367.490287	330190.670829	51.641793
3367.024598	329981.419838	51.646797
3366.170425	329781.700519	51.651802
3365.328398	329590.023876	51.656807
3364.984621	329373.572402	51.661812
3364.062665	329184.682438	51.666817
3363.316917	328980.590299	51.671821
3362.657603	328788.424466	51.676826
3361.815483	328590.635030	51.681831
3361.459107	328385.741403	51.686836
3360.515499	328200.747764	51.691841
3359.944181	327987.943639	51.696845
3359.372825	327792.197044	51.701850
3358.702806	327594.887046	51.706855
3358.138711	327391.296643	51.711860
3357.413440	327192.746832	51.716865
3356.594983	326996.298987	51.721869
3356.089210	326786.180011	51.726874
3355.543559	326589.280654	51.731879
3355.017041	326389.831756	51.736884
3354.057613	326187.981167	51.741889
3353.105057	325992.723238	51.746893
3352.925925	325783.033726	51.751898
3351.590395	325594.073223	51.756903
3351.326458	325399.596086	51.761908
3350.724909	325201.836529	51.766913
3350.053356	325008.823265	51.771917
3349.376410	324806.364443	51.776922
3348.639086	324619.242115	51.781927
3347.989918	324414.359161	51.786932
3347.115307	324220.026744	51.791937
3346.495388	324018.040746	51.796941
3346.241312	323825.009637	51.801946
3345.541316	323631.081084	51.806951
3344.892799	323419.575702	51.811956
3343.953398	323227.160838	51.816961
3343.099042	323026.100697	51.821965
3342.603328	322827.274894	51.826970
3341.931544	322643.498737	51.831975
3341.357376	322451.533608	51.836980
3340.481589	322264.096991	51.841985
3339.998756	322053.325901	51.846989
3339.396151	321861.669511	51.851994
3338.352527	321661.731000	51.856999
3338.088160	321475.520015	51.862004
3337.329066	321279.965997	51.867009
3336.539601	321069.393826	51.872013
3335.613305	320884.915854	51.877018
3335.304121	320685.444627	51.882023
3335.187272	320490.322019	51.887028
3333.939914	320292.042243	51.892033
3333.605865	320083.687342	51.897037
3332.510274	319895.236568	51.902042
3332.045555	319700.498297	51.907047
3331.458282	319493.862619	51.912052
3330.795630	319309.568930	51.917057
3330.027472	319111.465450	51.922061
3329.596390	318914.861455	51.927066
3328.465309	318721.092249	51.932071
3328.301577	318523.401190	51.937076
3327.053929	318331.966721	51.942081
3326.565189	318125.210601	51.947085
3325.912577	317931.415040	51.952090
3325.269520	317750.832781	51.957095
3324.625889	317545.958698	51.962100
3323.927862	317348.629811	51.967105
3323.385745	317146.005031	51.972109
3322.526571	316956.263343	51.977114
3321.693264	316769.496378	51.982119
3321.741778	316572.404345	51.987124
3320.750984	316375.094347	51.992129
3319.783044	316179.664622	51.997133
3319.406387	315980.576144	52.002138
3318.605915	315793.802161	52.007143
3317.699724	315598.590714	52.012148
3317.132582	315408.137856	52.017153
3316.606261	315213.094764	52.022157
3315.606614	315021.716517	52.027162
3315.129125	314824.424176	52.032167
3314.847812	314644.492079	52.037172
3313.843466	314437.606159	52.042177
3313.475928	314239.836977	52.047181
3312.993049	314049.470155	52.052186
3311.792789	313855.065851	52.057191
3311.430132	313663.126029	52.062196
3310.457126	313469.830954	52.067201
3309.925021	313273.537446	52.072205
3309.310136	313086.907523	52.077210
3308.594136	312888.019610	52.082215
3307.807015	312693.089516	52.087220
3307.064166	312498.406714	52.092225
3306.495881	312315.434938	52.097229
3305.876153	312119.815287	52.102234
3305.156475	311933.454623	52.107239
3304.188328	311733.509553	52.112244
3303.719893	311552.150449	52.117249
3303.248472	311362.108175	52.122253
3302.881752	311167.567286	52.127258
3301.694958	310981.228007	52.132263
3301.334507	310786.634552	52.137268
3300.688196	310602.399123	52.142273
3299.919028	310400.484946	52.147277
3299.358110	310204.521671	52.152282
3298.473969	310027.096544	52.157287
3297.711668	309830.527883	52.162292
3297.187997	309637.282501	52.167297
3296.657660	309451.626369	52.172301
3295.900532	309257.933470	52.177306
3294.959256	309068.980388	52.182311
3294.699387	308867.976192	52.187316
3293.725508	308684.400767	52.192321
3292.807232	308500.256044	52.197325
3292.664191	308310.971820	52.202330
3291.736330	308132.557699	52.207335
3291.035830	307936.154464	52.212340
3290.755731	307743.173153	52.217345
3289.762950	307553.691141	52.222349
3289.023787	307358.642779	52.227354
3288.150763	307184.624132	52.232359
3287.718980	306979.926176	52.237364
3287.231118	306793.520877	52.242369
3286.554841	306618.961044	52.247373
3286.046469	306437.218643	52.252378
3285.166092	306244.813883	52.257383
3284.562873	306042.611728	52.262388
3283.808182	305877.434616	52.267393
3283.341697	305669.989841	52.272397
3282.667402	305487.432030	52.277402
3281.742177	305295.083935	52.282407
3281.331899	305111.312442	52.287412
3280.858283	304914.690550	52.292417
3280.017890	304722.149978	52.297421
3279.534751	304535.562551	52.302426
3278.329924	304342.315128	52.307431
3277.898382	304154.929597	52.312436
3277.050779	303973.976095	52.317441
3276.780826	303766.319136	52.322445
3276.166122	303588.511547	52.327450
3275.073091	303406.450187	52.332455
3274.791420	303200.831550	52.337460
3273.885019	303015.913460	52.342465
3273.383870	302832.127943	52.347469
3272.665756	302638.062752	52.352474
3271.608269	302453.142397	52.357479
3271.226195	302263.811202	52.362484
3270.286940	302085.314635	52.367489
3269.900354	301887.732645	52.372493
3269.651450	301696.647984	52.377498
3268.411347	301519.267933	52.382503
3267.792762	301324.141221	52.387508
3267.123350	301137.477132	52.392513
3266.419349	300951.022027	52.397517
3265.781429	300758.164186	52.402522
3265.068682	300580.572341	52.407527
3264.354153	300385.561529	52.412532
3263.532182	300220.643399	52.417537
3262.863992	300027.764017	52.422541
3262.314101	299833.006642	52.427546
3261.820876	299656.168542	52.432551
3260.813683	299480.099155	52.437556
3260.360557	299294.086360	52.442561
3259.597087	299099.692993	52.447565
3259.247779	298924.308437	52.452570
3258.255578	298743.168056	52.457575
3257.832594	298549.866219	52.462580
3256.898258	298368.487100	52.467585
3256.230344	298187.829656	52.472589
3255.814837	298003.337551	52.477594
3255.079911	297821.085932	52.482599
3254.532116	297641.453083	52.487604
3253.742239	297463.233565	52.492609
3253.068879	297278.908853	52.497613
3252.189741	297089.421257	52.502618
3251.647801	296918.547412	52.507623
3251.249873	296728.830534	52.512628
3250.282458	296554.891229	52.517633
3249.612871	296360.480097	52.522637
3249.321113	296177.189044	52.527642
3248.601239	295999.237226	52.532647
3247.903291	295804.422561	52.537652
3247.187059	295622.853504	52.542657
3246.568783	295444.426716	52.547661
3245.864251	295248.288265	52.552666
3244.803891	295071.866591	52.557671
3244.524402	294874.412658	52.562676
3243.854554	294696.171655	52.567681
3243.013073	294525.827037	52.572685
3242.448343	294331.702998	52.577690
3241.508427	294160.227634	52.582695
3240.980505	293973.228298	52.587700
3240.431210	293801.639928	52.592705
3239.539684	293624.782884	52.597709
3239.070871	293434.386585	52.602714
3238.248168	293268.342015	52.607719
3237.710141	293074.671070	52.612724
3237.167913	292903.717591	52.617729
3236.664629	292705.202029	52.622733
3236.110738	292529.920654	52.627738
3235.026962	292349.502136	52.632743
3234.891881	292147.082272	52.637748
3234.142522	291964.904243	52.642753
3233.390718	291785.808041	52.647757
3232.594960	291598.492637	52.652762
3231.522241	291424.005641	52.657767
3231.086580	291234.366388	52.662772
3230.446820	291051.533674	52.667777
3229.952720	290874.993768	52.672781
3228.913258	290694.796270	52.677786
3228.393496	290508.735273	52.682791
3227.734555	290326.694595	52.687796
3226.976782	290156.078970	52.692801
3226.403924	289970.000540	52.697805
3226.166026	289773.121606	52.702810
3225.078533	289595.961654	52.707815
3224.698452	289407.662133	52.712820
3223.962623	289235.896437	52.717825
3222.913518	289052.159391	52.722829
3222.385266	288864.545129	52.727834
3221.692291	288689.486991	52.732839
3221.285050	288507.150679	52.737844
3220.630743	288330.099729	52.742849
3219.962512	288147.116864	52.747853
3219.363316	287945.047513	52.752858
3218.517026	287780.378567	52.757863
3217.778760	287597.279135	52.762868
3217.168586	287419.405736	52.767873
3216.203267	287232.037943	52.772877
3216.033140	287061.404050	52.777882
3215.016657	286879.901796	52.782887
3214.734644	286684.530539	52.787892
3213.761120	286520.314080	52.792897
3212.713089	286322.517013	52.797901
3212.275081	286149.760289	52.802906
3211.309956	285986.051630	52.807911
3210.645401	285793.185360	52.812916
3210.283016	285643.541445	52.817921
3209.590769	285470.009663	52.822925
3209.026200	285284.716820	52.827930
3208.104905	285113.105763	52.832935
3207.789470	284941.373321	52.837940
3206.932958	284759.004330	52.842945
3206.136474	284586.278190	52.847949
3205.542049	284416.703534	52.852954
3204.453707	284241.120067	52.857959
3204.493821	284068.184974	52.862964
3203.756591	283885.542082	52.867969
3202.819753	283719.943446	52.872973
3202.508117	283538.710249	52.877978
3201.724613	283369.623565	52.882983
3201.001013	283178.930309	52.887988
3200.412274	283009.583482	52.892993
3199.520964	282839.163869	52.897997
3199.274373	282661.230950	52.903002
3197.938690	282488.360179	52.908007
3197.452344	282310.363209	52.913012
3197.172995	282142.469803	52.918017
3196.162708	281962.518161	52.923021
3195.889177	281793.987034	52.928026
3194.765972	281612.907087	52.933031
3194.463406	281443.743756	52.938036
3193.720070	281272.969210	52.943041
3193.073189	281089.317874	52.948045
3192.965143	280905.784990	52.953050
3191.855294	280738.455588	52.958055
3191.246737	280559.611569	52.963060
3190.713912	280374.770474	52.968065
3189.864581	280196.804923	52.973069
3189.209230	280018.477558	52.978074
3188.305308	279844.671911	52.983079
3187.612288	279659.321176	52.988084
3187.038201	279493.027377	52.993089
3186.164888	279312.467682	52.998093
3185.680279	279130.038206	53.003098
3184.885305	278965.307373	53.008103
3184.614949	278796.418579	53.013108
3183.952178	278630.011341	53.018113
3183.009452	278445.922392	53.023117
3182.566641	278258.010475	53.028122
3181.907115	278086.076022	53.033127
3181.340573	277906.511795	53.038132
3180.450585	277738.714176	53.043137
3179.622747	277561.610750	53.048141
3179.567620	277375.241905	53.053146
3178.014076	277212.260875	53.058151
3177.533533	277038.184133	53.063156
3176.930892	276875.638408	53.068161
3176.172065	276702.115041	53.073165
3175.635169	276519.158716	53.078170
3174.709653	276346.807783	53.083175
3174.108271	276178.607845	53.088180
3173.541356	276000.928206	53.093185
3172.756110	275836.042772	53.098189
3172.308217	275655.899330	53.103194
3171.110615	275500.527908	53.108199
3170.743026	275335.729200	53.113204
3170.262142	275166.618791	53.118209
3169.573857	274988.092426	53.123213
3169.011011	274820.624968	53.128218
3167.874212	274656.762963	53.133223
3167.570509	274498.881564	53.138228
3166.749700	274325.724550	53.143233
3166.168592	274151.383542	53.148237
3165.788812	273984.345584	53.153242
3164.970752	273813.327508	53.158247
3164.166335	273656.213022	53.163252
3163.593998	273489.969616	53.168257
3162.856511	273313.157507	53.173261
3162.343006	273148.280114	53.178266
3161.506563	272978.130941	53.183271
3160.896274	272808.455372	53.188276
3160.384885	272635.988121	53.193281
3159.543166	272471.341007	53.198285
3159.341374	272289.172303	53.203290
3158.410330	272124.768581	53.208295
3157.630641	271949.109390	53.213300
3157.282160	271783.085439	53.218305
3156.403075	271609.734179	53.223309
3155.863714	271435.692486	53.228314
3154.766682	271267.698651	53.233319
3154.246358	271088.076441	53.238324
3153.475282	270925.175696	53.243329
3152.756502	270772.275758	53.248333
3152.449727	270595.243095	53.253338
3151.679459	270436.162562	53.258343
3151.102031	270260.140591	53.263348
3150.547161	270090.787786	53.268353
3149.616830	269915.356567	53.273357
3149.420159	269740.547885	53.278362
3148.499413	269582.026176	53.283367
3147.758074	269407.431100	53.288372
3146.869933	269238.487786	53.293377
3146.287653	269064.198720	53.298381
3145.483781	268903.315601	53.303386
3144.677802	268748.774451	53.308391
3144.047080	268566.216008	53.313396
3143.435489	268408.715340	53.318401
3142.915385	268240.783733	53.323405
3142.475947	268078.187738	53.328410
3141.292690	267925.412877	53.333415
3141.233660	267745.667617	53.338420
3140.567646	267581.426721	53.343425
3139.646548	267412.234475	53.348429
3139.379277	267235.731334	53.353434
3138.441198	267076.576352	53.358439
3137.852854	266891.439491	53.363444
3137.054645	266730.861742	53.368449
3136.093415	266565.343556	53.373453
3135.960387	266400.967788	53.378458
3134.918934	266240.148551	53.383463
3134.541719	266056.837793	53.388468
3133.727740	265890.659855	53.393473
3133.025247	265722.070339	53.398477
3132.498166	265555.363242	53.403482
3131.723083	265381.793606	53.408487
3131.203042	265216.995639	53.413492
3130.486532	265044.537476	53.418497
3129.739473	264879.419019	53.423501
3129.324338	264700.189757	53.428506
3128.433167	264546.733138	53.433511
3127.759394	264371.747182	53.438516
3127.239371	264201.295751	53.443521
3126.202518	264041.164313	53.448525
3125.806440	263861.983380	53.453530
3124.709340	263703.313302	53.458535
3124.208475	263527.103405	53.463540
3123.570150	263371.951866	53.468545
3122.677419	263212.129089	53.473549
3122.368237	263050.202084	53.478554
3121.316845	262895.829231	53.483559
3120.603552	262736.182035	53.488564
3120.108921	262568.146855	53.493569
3118.895412	262417.569132	53.498573
3118.699996	262249.766921	53.503578
3118.274107	262089.412410	53.508583
3117.674895	261937.871809	53.513588
3116.966108	261773.945800	53.518593
3116.214862	261608.396661	53.523597
3115.733425	261441.760741	53.528602
3114.663348	261279.980537	53.533607
3114.772793	261114.524692	53.538612
3113.877547	260941.027315	53.543617
3113.103790	260787.630322	53.548621
3112.525798	260619.685841	53.553626
3111.469002	260456.044867	53.558631
3110.841827	260282.225340	53.563636
3110.245552	260121.898895	53.568641
3109.464865	259961.448923	53.573645
3109.172494	259808.663935	53.578650
3108.081364	259637.414077	53.583655
3107.418184	259488.024214	53.588660
3106.954750	259309.875397	53.593665
3106.031817	259164.601642	53.598669
3105.989797	258998.101439	53.603674
3104.806206	258839.473191	53.608679
3104.564921	258678.403854	53.613684
3103.662173	258508.856750	53.618689
3102.978260	258353.231315	53.623693
3102.648123	258180.435863	53.628698
3101.732440	258029.253188	53.633703
3100.828923	257864.672819	53.638708
3100.356464	257690.193932	53.643713
3099.577373	257540.619876	53.648717
3099.075111	257376.129163	53.653722
3098.195560	257221.121198	53.658727
3097.765928	257056.517356	53.663732
3097.035834	256889.261648	53.668737
3096.113371	256729.574831	53.673741
3095.757842	256570.791638	53.678746
3094.906189	256410.609971	53.683751
3094.504566	256255.094115	53.688756
3093.733768	256085.477018	53.693761
3092.818597	255934.881439	53.698765
3092.374622	255761.265467	53.703770
3091.616079	255600.738609	53.708775
3091.147065	255442.458101	53.713780
3090.367773	255283.233601	53.718785
3089.720871	255129.438235	53.723789
3089.112412	254960.738659	53.728794
3088.492015	254812.643969	53.733799
3087.656120	254641.230214	53.738804
3087.443511	254488.283431	53.743809
3086.585360	254321.712212	53.748813
3085.666000	254148.656745	53.753818
3084.872138	253998.374500	53.758823
3084.735448	253827.130953	53.763828
3083.819573	253675.824128	53.768833
3083.190155	253508.784488	53.773837
3082.699907	253344.422460	53.778842
3081.666393	253193.643983	53.783847
3081.114440	253024.809842	53.788852
3080.519393	252865.379927	53.793857
3079.749264	252707.454933	53.798861
3079.215752	252537.701525	53.803866
3078.500663	252389.343603	53.808871
3077.961904	252211.849449	53.813876
3077.076193	252047.576657	53.818881
3076.230384	251890.683038	53.823885
3076.012891	251726.966933	53.828890
3074.981725	251577.742925	53.833895
3074.154537	251407.731493	53.838900
3073.361768	251251.517664	53.843905
3072.784457	251095.422680	53.848909
3072.852836	250928.758917	53.853914
3071.500804	250780.299458	53.858919
3070.998053	250625.542840	53.863924
3070.485232	250471.602887	53.868929
3069.596799	250312.170844	53.873933
3069.086906	250143.129150	53.878938
3067.886052	249999.281362	53.883943
3067.630022	249843.747919	53.888948
3067.094637	249691.365729	53.893953
3066.410523	249530.730677	53.898957
3065.903602	249364.745295	53.903962
3065.032534	249202.917785	53.908967
3064.296059	249047.537563	53.913972
3063.830786	248888.167315	53.918977
3062.837562	248736.877165	53.923981
3062.506575	248569.973477	53.928986
3061.913571	248424.553908	53.933991
3061.190775	248254.758507	53.938996
3060.169633	248109.381535	53.944001
3059.465754	247947.987289	53.949005
3058.966171	247797.307542	53.954010
3058.028286	247645.118425	53.959015
3057.381853	247483.359073	53.964020
3057.040069	247339.123174	53.969025
3056.028374	247183.253662	53.974029
3055.524025	247022.236313	53.979034
3054.732513	246867.452794	53.984039
3054.292231	246715.491492	53.989044
3053.638012	246573.725064	53.994049
3053.051106	246417.254377	53.999053
3052.571890	246257.736397	54.004058
3051.669099	246107.707950	54.009063
3051.077534	245943.242298	54.014068
3050.604880	245779.445595	54.019073
3049.796855	245635.921868	54.024077
3049.302497	245478.648158	54.029082
3048.587640	245315.781639	54.034087
3047.738770	245160.703513	54.039092
3047.136594	245002.301472	54.044097
3046.605360	244854.456561	54.049101
3045.833412	244691.472508	54.054106
3044.726999	244541.758139	54.059111
3044.153720	244384.803789	54.064116
3043.874434	244239.491694	54.069121
3042.956702	244080.809650	54.074125
3042.755342	243917.889041	54.079130
3041.656158	243756.638652	54.084135
3041.354192	243594.218214	54.089140
3040.695350	243443.874039	54.094145
3039.869088	243287.903272	54.099149
3039.203900	243130.863132	54.104154
3038.231733	242983.141073	54.109159
3037.932716	242823.802433	54.114164
3037.226769	242669.519549	54.119169
3036.447854	242510.282729	54.124173
3035.766104	242351.998403	54.129178
3035.058665	242195.602754	54.134183
3034.326521	242042.114213	54.139188
3033.716673	241894.819941	54.144193
3033.089440	241747.503134	54.149197
3032.723146	241580.257183	54.154202
3031.680298	241436.749865	54.159207
3031.329343	241280.171649	54.164212
3030.619608	241118.506551	54.169217
3029.606617	240967.457516	54.174221
3029.085113	240804.999112	54.179226
3028.299940	240661.604736	54.184231
3027.731923	240503.712278	54.189236
3027.229336	240361.572236	54.194241
3026.539481	240205.609308	54.199245
3025.973252	240038.117075	54.204250
3025.147580	239895.850491	54.209255
3024.491555	239735.732139	54.214260
3023.961433	239590.134246	54.219265
3023.263472	239436.439977	54.224269
3022.790453	239265.852937	54.229274
3021.837921	239118.718257	54.234279
3021.071369	238961.623279	54.239284
3020.250028	238813.475130	54.244289
3019.663484	238654.213099	54.249293
3019.438045	238512.795431	54.254298
3018.660113	238358.529626	54.259303
3017.857303	238203.045700	54.264308
3017.364689	238055.279426	54.269313
3016.730073	237898.572502	54.274317
3016.276284	237737.813876	54.279322
3015.467414	237585.260148	54.284327
3014.623201	237421.609975	54.289332
3013.882938	237267.441613	54.294337
3012.938494	237106.277781	54.299341
3012.581639	236947.440246	54.304346
3011.803233	236800.866803	54.309351
3011.024062	236649.812073	54.314356
3010.917455	236490.324486	54.319361
3009.538734	236346.316672	54.324365
3009.234259	236182.201031	54.329370
3008.633430	236030.864332	54.334375
3007.991464	235878.464897	54.339380
3007.073169	235727.968260	54.344385
3006.284281	235577.247654	54.349389
3005.913482	235425.136995	54.354394
3005.040158	235269.923185	54.359399
3004.386027	235119.665729	54.364404
3003.995566	234967.227845	54.369409
3003.072689	234817.446253	54.374413
3002.577869	234664.337839	54.379418
3001.736626	234522.691994	54.384423
3001.256365	234363.852522	54.389428
3000.693763	234215.542595	54.394433
2999.703912	234056.809740	54.399437
2999.339514	233911.982797	54.404442
2998.454323	233758.504702	54.409447
2998.024038	233608.697893	54.414452
2997.501675	233452.794793	54.419457
2996.723698	233306.353662	54.424461
2996.042561	233148.133601	54.429466
2995.235700	233002.792403	54.434471
2994.731537	232849.459137	54.439476
2993.968359	232699.451804	54.444481
2993.433835	232561.375961	54.449485
2992.372929	232393.032200	54.454490
2991.999413	232247.623558	54.459495
2991.208964	232093.776650	54.464500
2990.382923	231947.421601	54.469505
2989.514137	231797.432416	54.474509
2988.891757	231645.647561	54.479514
2988.201995	231518.139262	54.484519
2988.026193	231361.879189	54.489524
2987.411159	231210.272119	54.494529
2986.635243	231059.556482	54.499533
2986.248793	230913.693648	54.504538
2985.188525	230758.287546	54.509543
2984.564682	230611.266051	54.514548
2983.910432	230457.604003	54.519553
2983.246330	230310.716678	54.524557
2982.617121	230168.076222	54.529562
2981.693286	230019.371760	54.534567
2981.445729	229860.146568	54.539572
2981.069200	229714.971567	54.544577
2980.081955	229569.486086	54.549581
2979.201036	229417.287562	54.554586
2979.143137	229261.267066	54.559591
2978.241780	229103.648966	54.564596
2977.230585	228954.323573	54.569601
2976.383875	228804.921474	54.574605
2975.999571	228660.258668	54.579610
2975.365256	228518.512832	54.584615
2974.821542	228360.610303	54.589620
2974.216118	228203.965442	54.594625
2973.658393	228056.632183	54.599629
2972.846171	227908.983004	54.604634
2972.095438	227756.028394	54.609639
2971.038730	227608.596664	54.614644
2970.593232	227465.065846	54.619649
2970.205309	227312.742052	54.624653
2969.508302	227151.199610	54.629658
2968.422725	227012.404808	54.634663
2967.999631	226850.004829	54.639668
2967.452765	226706.975105	54.644673
2966.564188	226561.504546	54.649677
2966.126718	226410.857920	54.654682
2965.225227	226265.517228	54.659687
2964.577816	226106.056743	54.664692
2964.247545	225969.321010	54.669697
2962.944686	225829.136775	54.674701
2962.480279	225677.286366	54.679706
2961.737571	225545.530537	54.684711
2961.016036	225388.603781	54.689716
2960.561785	225253.378313	54.694721
2959.986714	225114.862331	54.699725
2959.434846	224960.646546	54.704730
2958.702958	224828.839246	54.709735
2957.873113	224668.519337	54.714740
2957.585563	224521.047734	54.719745
2956.514747	224380.129116	54.724749
2956.094807	224228.083434	54.729754
2955.035991	224083.433519	54.734759
2954.586735	223937.541665	54.739764
2954.155503	223796.968382	54.744769
2953.370514	223661.594279	54.749773
2952.606368	223507.822268	54.754778
2952.305428	223364.975921	54.759783
2951.399475	223212.754535	54.764788
2950.838552	223064.794266	54.769793
2949.912119	222920.405594	54.774797
2949.669930	222761.333166	54.779802
2948.797414	222628.749822	54.784807
2947.970350	222479.381601	54.789812
2947.355876	222326.632078	54.794817
2946.442494	222191.369970	54.799821
2945.858824	222027.095721	54.804826
2945.074261	221898.687803	54.809831
2944.571367	221750.058928	54.814836
2943.976806	221608.573477	54.819841
2943.388065	221472.077392	54.824845
2942.619266	221313.536881	54.829850
2941.915952	221177.492275	54.834855
2941.327371	221038.260087	54.839860
2940.825136	220900.580223	54.844865
2940.021457	220745.979866	54.849869
2939.572179	220594.569747	54.854874
2938.681913	220462.642212	54.859879
2937.925613	220314.069029	54.864884
2937.339699	220170.828261	54.869889
2936.379835	220035.220972	54.874893
2935.745634	219883.599726	54.879898
2935.417790	219755.874218	54.884903
2934.397610	219604.403762	54.889908
2934.219097	219455.562631	54.894913
2933.366727	219325.247762	54.899917
2932.840784	219173.356266	54.904922
2931.973369	219037.621631	54.909927
2931.409744	218881.357856	54.914932
2930.792597	218738.443077	54.919937
2929.797604	218607.210124	54.924941
2929.420406	218451.414206	54.929946
2928.804793	218325.009694	54.934951
2927.881377	218176.938317	54.939956
2927.343348	218040.262387	54.944961
2926.318564	217895.873613	54.949965
2926.099556	217762.622738	54.954970
2925.471275	217624.701726	54.959975
2924.619051	217467.913935	54.964980
2923.990708	217338.254587	54.969985
2923.252719	217192.192547	54.974989
2922.845374	217051.373678	54.979994
2922.084026	216913.742437	54.984999
2921.430742	216767.947909	54.990004
2920.576908	216622.427285	54.995009
2919.919195	216487.746292	55.000013
2919.329791	216349.936202	55.005018
2918.330863	216212.891304	55.010023
2918.092949	216065.034085	55.015028
2917.457894	215932.425368	55.020033
2916.391654	215792.642573	55.025037
2916.063864	215653.010452	55.030042
2915.485244	215517.707865	55.035047
2914.941826	215372.980832	55.040052
2914.359370	215229.698613	55.045057
2913.310371	215077.007817	55.050061
2912.728882	214932.275024	55.055066
2912.353480	214798.940073	55.060071
2911.355705	214663.374618	55.065076
2910.778264	214518.794816	55.070081
2910.000541	214381.005808	55.075085
2909.526193	214233.902808	55.080090
2908.959200	214090.442374	55.085095
2907.950860	213962.771581	55.090100
2907.389066	213815.836091	55.095105
2906.603122	213688.028790	55.100109
2905.973029	213544.235867	55.105114
2905.226283	213408.480492	55.110119
2904.530664	213268.020607	55.115124
2904.382855	213118.539134	55.120129
2903.387485	212990.091758	55.125133
2903.022057	212847.340349	55.130138
2902.465279	212700.368378	55.135143
2901.088905	212558.426796	55.140148
2900.631532	212427.057001	55.145153
2900.113804	212284.280032	55.150157
2899.744734	212152.082225	55.155162
2898.779118	212008.714926	55.160167
2898.107432	211871.563535	55.165172
2897.511299	211726.560108	55.170177
2896.561835	211594.493526	55.175181
2895.998023	211458.229617	55.180186
2895.456226	211323.731677	55.185191
2894.730913	211188.843061	55.190196
2894.250572	211044.650157	55.195201
2893.004672	210908.979078	55.200205
2892.923741	210771.711066	55.205210
2892.139877	210644.660403	55.210215
2891.447409	210511.460811	55.215220
2891.077257	210364.642852	55.220225
2889.968345	210224.649635	55.225229
2889.359645	210085.583006	55.230234
2888.875117	209954.668087	55.235239
2887.932731	209822.642283	55.240244
2887.272015	209675.235579	55.245249
2886.181181	209542.393864	55.250253
2886.062139	209395.156609	55.255258
2885.135880	209275.729541	55.260263
2884.492165	209143.976080	55.265268
2884.084892	209006.407264	55.270273
2883.487574	208890.276146	55.275277
2882.908322	208742.387865	55.280282
2882.173626	208608.664508	55.285287
2881.671572	208467.981010	55.290292
2880.900230	208338.374936	55.295297
2880.039640	208190.367088	55.300301
2879.600881	208056.636269	55.305306
2878.577190	207916.227552	55.310311
2877.988766	207781.019244	55.315316
2877.678392	207647.167188	55.320321
2876.846803	207512.316162	55.325325
2876.246544	207374.361611	55.330330
2875.414971	207245.772854	55.335335
2874.810587	207109.690427	55.340340
2874.467481	206973.401490	55.345345
2873.352074	206839.716889	55.350349
2872.885925	206692.973874	55.355354
2871.963136	206567.188202	55.360359
2871.483067	206432.767580	55.365364
2871.165821	206297.443336	55.370369
2870.286315	206157.512275	55.375373
2869.326485	206020.788663	55.380378
2868.874533	205883.284985	55.385383
2868.417963	205755.289149	55.390388
2867.752459	205606.531420	55.395393
2866.831198	205481.625967	55.400397
2866.064569	205338.128281	55.405402
2865.787116	205215.895840	55.410407
2864.704245	205068.147337	55.415412
2864.201686	204933.364653	55.420417
2863.446574	204791.253680	55.425421
2862.660590	204673.353531	55.430426
2861.924394	204539.588695	55.435431
2861.416204	204404.579065	55.440436
2860.996397	204277.356979	55.445441
2860.193376	204152.066619	55.450445
2859.422918	204005.658541	55.455450
2858.921284	203868.256605	55.460455
2858.158199	203740.784642	55.465460
2857.814341	203597.567965	55.470465
2856.987508	203472.651929	55.475469
2856.628871	203331.143565	55.480474
2855.576501	203200.002609	55.485479
2854.856713	203060.880979	55.490484
2854.272331	202915.973375	55.495489
2853.105046	202806.002143	55.500493
2853.060407	202662.727731	55.505498
2852.344647	202533.825698	55.510503
2851.558080	202405.635099	55.515508
2850.933291	202261.791834	55.520513
2850.108095	202123.809099	55.525517
2849.630713	202003.015069	55.530522
2848.933537	201869.810315	55.535527
2848.379804	201736.188670	55.540532
2847.779050	201599.838769	55.545537
2846.958938	201462.964011	55.550541
2846.380258	201324.524286	55.555546
2845.652582	201201.201067	55.560551
2844.777946	201059.194806	55.565556
2844.025853	200925.237499	55.570561
2843.172191	200789.082366	55.575565
2842.906499	200671.693623	55.580570
2842.263818	200534.971245	55.585575
2841.550873	200410.680344	55.590580
2841.179354	200268.711000	55.595585
2839.958729	200154.490508	55.600589
2839.482496	200017.603097	55.605594
2838.971918	199880.097932	55.610599
2838.239999	199760.138131	55.615604
2837.872429	199614.085071	55.620609
2836.721233	199490.629201	55.625613
2836.304436	199358.989561	55.630618
2835.383177	199231.311297	55.635623
2834.793148	199105.769604	55.640628
2834.360908	198972.466372	55.645633
2833.361546	198847.180985	55.650637
2833.026527	198703.861141	55.655642
2832.613610	198581.410267	55.660647
2831.635724	198448.054782	55.665652
2830.817090	198312.243954	55.670657
2830.330635	198192.783256	55.675661
2829.711623	198047.257856	55.680666
2828.806905	197927.189579	55.685671
2828.259296	197799.481044	55.690676
2827.945259	197656.364318	55.695681
2827.155595	197537.500289	55.700685
2826.619274	197395.208411	55.705690
2825.889195	197266.308502	55.710695
2825.401450	197124.391410	55.715700
2824.816859	196987.554431	55.720705
2823.997097	196861.672733	55.725709
2823.428879	196720.723829	55.730714
2822.553432	196584.582926	55.735719
2821.860246	196444.952463	55.740724
2821.521841	196321.235359	55.745729
2820.306347	196183.240701	55.750733
2820.089485	196048.994649	55.755738
2819.525356	195908.149115	55.760743
2818.632847	195772.203930	55.765748
2817.688976	195640.758906	55.770753
2816.748429	195518.704180	55.775757
2816.330299	195374.159693	55.780762
2815.787695	195251.495448	55.785767
2815.072361	195119.786542	55.790772
2814.588457	194982.150069	55.795777
2813.755239	194861.721335	55.800781
2813.293675	194725.341706	55.805786
2812.511948	194592.092356	55.810791
2811.561737	194462.178274	55.815796
2811.218956	194323.834152	55.820801
2810.515243	194205.269622	55.825805
2810.328988	194063.542317	55.830810
2809.046901	193941.380084	55.835815
2808.095005	193812.180490	55.840820
2807.951830	193673.501182	55.845825
2807.231151	193545.576209	55.850829
2806.308743	193411.830609	55.855834
2805.722896	193288.325518	55.860839
2805.150195	193156.815484	55.865844
2804.805644	193023.691941	55.870849
2804.108189	192887.558264	55.875853
2803.437657	192755.759425	55.880858
2802.713263	192622.226348	55.885863
2801.935607	192497.328581	55.890868
2801.458620	192352.433170	55.895873
2800.542012	192236.286348	55.900877
2799.902457	192094.560126	55.905882
2798.951860	191962.247945	55.910887
2798.399137	191834.987876	55.915892
2797.514872	191695.566316	55.920897
2796.889104	191586.868981	55.925901
2796.684176	191460.318205	55.930906
2795.954797	191336.280943	55.935911
2795.121167	191199.753670	55.940916
2794.780752	191067.932554	55.945921
2793.804324	190936.594218	55.950925
2793.076805	190803.499210	55.955930
2792.424698	190677.721071	55.960935
2791.884356	190548.668483	55.965940
2791.491346	190412.582578	55.970945
2790.818492	190290.053086	55.975949
2790.306838	190152.638083	55.980954
2789.371772	190015.710387	55.985959
2788.506224	189893.148818	55.990964
2787.922409	189758.558115	55.995969
2787.299706	189625.869636	56.000973
2786.913866	189491.477344	56.005978
2786.230498	189364.867920	56.010983
2785.271328	189237.564605	56.015988
2784.865129	189093.927330	56.020993
2783.411860	188970.863269	56.025997
2783.265850	188839.679094	56.031002
2782.824193	188714.063659	56.036007
2781.934413	188578.786872	56.041012
2781.360279	188452.137157	56.046017
2780.941336	188322.193560	56.051021
2780.255642	188187.254530	56.056026
2779.387062	188058.108052	56.061031
2778.911395	187940.184344	56.066036
2778.543668	187787.168679	56.071041
2777.616915	187666.607276	56.076045
2776.803726	187520.609353	56.081050
2776.376281	187395.427770	56.086055
2775.355955	187259.399445	56.091060
2774.718765	187129.341084	56.096065
2773.946228	187003.859002	56.101069
2773.711189	186863.483767	56.106074
2773.043548	186738.850887	56.111079
2772.127377	186595.429313	56.116084
2771.621107	186459.385547	56.121089
2770.500252	186332.255741	56.126093
2770.147779	186202.536566	56.131098
2769.561431	186076.938481	56.136103
2768.856002	185957.593239	56.141108
2768.017158	185820.484542	56.146113
2767.405957	185692.461615	56.151117
2767.076743	185549.446511	56.156122
2766.020310	185430.654391	56.161127
2765.498325	185309.691604	56.166132
2765.074599	185161.400540	56.171137
2763.936788	185041.884486	56.176141
2763.517871	184901.353602	56.181146
2762.801086	184762.931197	56.186151
2762.060452	184646.241041	56.191156
2761.644108	184516.231504	56.196161
2760.856962	184399.231325	56.201165
2760.480147	184255.070235	56.206170
2759.939917	184127.333108	56.211175
2759.091906	183986.669517	56.216180
2758.581248	183847.339539	56.221185
2757.610196	183722.712156	56.226189
2757.038646	183570.404473	56.231194
2756.608594	183449.292224	56.236199
2755.815670	183311.026318	56.241204
2754.965213	183180.377069	56.246209
2754.253011	183050.126097	56.251213
2753.617473	182909.597646	56.256218
2752.744244	182785.911476	56.261223
2752.163313	182657.879736	56.266228
2751.734449	182528.730301	56.271233
2751.047733	182400.614302	56.276237
2750.205291	182267.269712	56.281242
2749.572028	182129.592828	56.286247
2749.012846	182010.603897	56.291252
2748.032383	181870.909369	56.296257
2747.442194	181753.808692	56.301261
2746.896307	181617.824135	56.306266
2746.237269	181489.159452	56.311271
2745.531659	181364.662097	56.316276
2745.060126	181219.393846	56.321281
2744.411627	181107.977427	56.326285
2743.782621	180962.645941	56.331290
2742.890631	180848.075972	56.336295
2742.000618	180722.375815	56.341300
2741.593833	180586.143510	56.346305
2740.957665	180449.808048	56.351309
2740.688251	180322.179066	56.356314
2739.721740	180189.636463	56.361319
2738.846685	180063.859549	56.366324
2738.570762	179931.068442	56.371329
2737.682090	179800.880632	56.376333
2736.973181	179674.569753	56.381338
2736.637890	179543.417405	56.386343
2735.419651	179408.360417	56.391348
2735.186829	179283.565268	56.396353
2734.214939	179152.349608	56.401357
2733.684960	179014.908025	56.406362
2732.898995	178893.267091	56.411367
2732.143716	178767.106183	56.416372
2731.603938	178636.383346	56.421377
2730.967070	178509.962780	56.426381
2730.277231	178388.015532	56.431386
2729.773960	178253.981031	56.436391
2729.312017	178127.483033	56.441396
2728.656761	177983.844866	56.446401
2728.038375	177862.015026	56.451405
2727.305334	177723.503254	56.456410
2726.775997	177595.160525	56.461415
2725.789967	177464.804580	56.466420
2725.639054	177321.788365	56.471425
2724.679594	177194.405349	56.476429
2724.027069	177062.954869	56.481434
2723.314995	176925.281901	56.486439
2722.534409	176798.100715	56.491444
2721.817366	176652.937939	56.496449
2721.172268	176538.442351	56.501453
2720.670669	176398.804522	56.506458
2720.191574	176269.542188	56.511463
2719.157865	176143.242567	56.516468
2718.664830	176003.795508	56.521473
2717.982687	175874.057834	56.526477
2717.479371	175744.559337	56.531482
2716.671581	175607.300229	56.536487
2715.929880	175480.765622	56.541492
2715.189261	175338.193119	56.546497
2714.390154	175220.367916	56.551501
2714.133173	175078.393797	56.556506
2713.648074	174952.634170	56.561511
2712.597350	174825.896186	56.566516
2712.190594	174681.021950	56.571521
2711.467057	174548.929450	56.576525
2710.730733	174426.823258	56.581530
2710.072373	174284.292311	56.586535
2709.100906	174148.361337	56.591540
2708.821662	174018.222393	56.596545
2708.139099	173903.612984	56.601549
2707.412651	173759.059789	56.606554
2706.899774	173633.474018	56.611559
2706.102095	173492.277913	56.616564
2705.699749	173353.283477	56.621569
2704.921151	173222.641196	56.626573
2704.477715	173087.673052	56.631578
2703.523523	172963.838055	56.636583
2702.947020	172829.476886	56.641588
2702.316777	172684.492664	56.646593
2701.529013	172559.004700	56.651597
2701.000550	172418.876202	56.656602
2700.571521	172274.001504	56.661607
2699.356325	172158.680294	56.666612
2698.645218	172010.379356	56.671617
2697.896382	171877.295042	56.676621
2697.601077	171752.125877	56.681626
2696.813438	171611.469025	56.686631
2696.529880	171492.301433	56.691636
2695.958343	171344.209814	56.696641
2695.025202	171223.022156	56.701645
2694.477178	171066.241982	56.706650
2694.020786	170935.314621	56.711655
2693.076784	170803.053343	56.716660
2692.499597	170647.894548	56.721665
2691.577299	170527.851873	56.726669
2691.087159	170382.955707	56.731674
2690.034068	170248.831489	56.736679
2689.225824	170120.060911	56.741684
2689.205155	169990.199517	56.746689
2688.074442	169852.235767	56.751693
2687.357428	169724.889056	56.756698
2687.081161	169589.079908	56.761703
2686.171790	169466.418844	56.766708
2685.962741	169325.195393	56.771713
2685.125127	169190.875410	56.776717
2684.726412	169052.137311	56.781722
2684.165466	168904.371273	56.786727
2683.187650	168777.755714	56.791732
2682.845131	168636.530515	56.796737
2681.750844	168490.427405	56.801741
2680.954043	168360.058668	56.806746
2680.665423	168217.949058	56.811751
2679.801446	168091.699238	56.816756
2679.226070	167934.529250	56.821761
2678.409283	167810.676247	56.826765
2677.703486	167673.937392	56.831770
2677.208567	167542.010434	56.836775
2676.484448	167407.373593	56.841780
2676.121767	167263.549927	56.846785
2675.218487	167134.918938	56.851789
2674.489458	166985.826410	56.856794
2674.056550	166853.879326	56.861799
2673.252789	166720.986912	56.866804
2673.010722	166580.376559	56.871809
2672.162676	166440.091617	56.876813
2671.614577	166291.113067	56.881818
2670.858134	166152.289706	56.886823
2669.737531	166006.785332	56.891828
2669.493154	165861.549608	56.896833
2668.551084	165737.926757	56.901837
2667.873515	165586.682764	56.906842
2667.477149	165460.761911	56.911847
2666.397054	165322.793995	56.916852
2666.154653	165178.959314	56.921857
2665.443629	165052.759105	56.926861
2664.907513	164896.943490	56.931866
2663.867231	164773.186848	56.936871
2663.256999	164632.019170	56.941876
2662.664305	164494.333164	56.946881
2662.047644	164350.395719	56.951885
2661.461259	164211.298419	56.956890
2660.560763	164068.602250	56.961895
2660.029241	163947.806646	56.966900
2659.288899	163798.474462	56.971905
2658.533453	163663.271320	56.976909
2658.046411	163528.305879	56.981914
2657.533387	163384.508402	56.986919
2656.842398	163261.210134	56.991924
2656.294838	163117.164896	56.996929
2655.421847	162975.422250	57.001933
2654.894352	162836.041161	57.006938
2654.399431	162690.501697	57.011943
2653.493205	162540.921259	57.016948
2653.264660	162402.435342	57.021953
2652.334884	162264.137339	57.026957
2651.571007	162118.617368	57.031962
2650.946660	161982.662323	57.036967
2649.932829	161840.921030	57.041972
2649.322649	161697.285529	57.046977
2648.638504	161569.325929	57.051981
2648.014380	161429.927464	57.056986
2647.631984	161299.225674	57.061991
2646.834380	161161.038136	57.066996
2646.303569	161017.354656	57.072001
2645.641179	160881.498829	57.077005
2645.279125	160733.759510	57.082010
2644.526528	160598.135192	57.087015
2643.703222	160463.870235	57.092020
2643.293946	160307.571228	57.097025
2642.432365	160164.337732	57.102029
2641.582073	160019.030742	57.107034
2641.039102	159883.795499	57.112039
2640.188516	159735.819919	57.117044
2640.054139	159603.673917	57.122049
2639.191121	159460.151110	57.127053
2638.624507	159310.683025	57.132058
2638.002380	159160.207325	57.137063
2636.946662	159017.632207	57.142068
2636.498560	158875.762322	57.147073
2635.979880	158738.811393	57.152077
2634.924658	158593.008845	57.157082
2634.400635	158449.767017	57.162087
2633.704363	158310.900844	57.167092
2633.481458	158162.692641	57.172097
2632.318016	158018.791135	57.177101
2631.736880	157876.984542	57.182106
2631.276452	157734.422074	57.187111
2630.323478	157591.480583	57.192116
2629.913626	157457.415930	57.197121
2629.202614	157315.263558	57.202125
2628.696386	157163.252664	57.207130
2627.967672	157032.914060	57.212135
2627.034003	156889.552920	57.217140
2626.672622	156745.275411	57.222145
2625.868073	156602.810293	57.227149
2625.347904	156447.537753	57.232154
2624.797878	156306.215769	57.237159
2623.562466	156166.973325	57.242164
2623.209199	156031.074755	57.247169
2622.546366	155879.196074	57.252173
2621.772908	155741.610995	57.257178
2621.031771	155596.991732	57.262183
2620.640564	155441.614364	57.267188
2620.043039	155309.087856	57.272193
2619.366027	155168.083093	57.277197
2618.474412	155021.812196	57.282202
2618.245544	154877.063997	57.287207
2617.392452	154738.148195	57.292212
2616.896549	154586.223444	57.297217
2616.299550	154432.904437	57.302221
2615.610877	154284.570770	57.307226
2614.670220	154152.573497	57.312231
2614.034780	154000.571814	57.317236
2613.781022	153843.489450	57.322241
2613.008465	153710.259729	57.327245
2612.244722	153552.420607	57.332250
2611.786673	153427.658564	57.337255
2610.950885	153195.638704	57.342260
2610.584433	153053.500492	57.347265
2609.765842	152903.070841	57.352269
2609.415594	152733.260100	57.357274
2608.532179	152593.455565	57.362279
2607.766279	152448.942791	57.367284
2607.689747	152283.679511	57.372289
2606.277030	152133.639840	57.377293
2605.525612	151979.098268	57.382298
2605.216553	151825.745654	57.387303
2604.225805	151699.689101	57.392308
2603.841042	151525.886295	57.397313
2602.804812	151388.665847	57.402317
2602.496509	151240.438051	57.407322
2601.803202	151089.869728	57.412327
2601.446385	150917.540089	57.417332
2600.461716	150779.818337	57.422337
2599.889174	150621.492681	57.427341
2599.330970	150467.728350	57.432346
2598.795266	150319.922061	57.437351
2597.546184	150178.025112	57.442356
2597.406074	150005.246543	57.447361
2596.515022	149859.633879	57.452365
2595.829027	149705.550249	57.457370
2595.212333	149574.740127	57.462375
2594.501791	149414.688322	57.467380
2593.989443	149252.178419	57.472385
2593.137251	149097.780875	57.477389
2592.389122	148964.668257	57.482394
2591.847934	148800.195275	57.487399
2591.306891	148648.648277	57.492404
2590.441724	148482.029588	57.497409
2589.878854	148351.050699	57.502413
2589.127450	148202.284290	57.507418
2588.700119	148041.139616	57.512423
2587.695020	147885.107286	57.517428
2587.496733	147755.458329	57.522433
2586.610314	147586.674485	57.527437
2585.635869	147449.918520	57.532442
2585.589442	147269.120687	57.537447
2584.433620	147151.927814	57.542452
2583.919428	146971.015176	57.547457
2583.215793	146846.279218	57.552461
2582.366139	146685.030429	57.557466
2582.124599	146519.581333	57.562471
2580.911099	146397.863551	57.567476
2580.793264	146210.779813	57.572481
2580.194541	146103.541988	57.577485
2579.204018	145916.153506	57.582490
2578.707754	145778.185294	57.587495
2577.794866	145614.575626	57.592500
2577.902788	145473.323334	57.597505
2576.850062	145298.884985	57.602509
2576.228069	145171.258081	57.607514
2575.619830	144980.256469	57.612519
2574.233409	144870.402846	57.617524
2574.172089	144684.666277	57.622529
2573.411971	144529.869817	57.627533
2572.811041	144395.380735	57.632538
2572.115764	144236.191415	57.637543
2571.431204	144088.920634	57.642548
2570.847286	143912.408031	57.647553
2570.197998	143796.786705	57.652557
2569.234848	143614.973480	57.657562
2569.041465	143467.322860	57.662567
2568.225690	143306.200549	57.667572
2567.836365	143163.296715	57.672577
2567.058299	142999.476176	57.677581
2565.992292	142844.685819	57.682586
2565.745050	142675.433348	57.687591
2565.072014	142532.031027	57.692596
2564.241203	142358.705011	57.697601
2563.449157	142231.117219	57.702605
2562.981848	142060.022467	57.707610
2562.420939	141913.149137	57.712615
2561.701782	141749.580094	57.717620
2560.834153	141576.404134	57.722625
2560.396671	141447.708824	57.727629
2559.752543	141283.075793	57.732634
2558.735017	141131.869585	57.737639
2558.510008	140984.007277	57.742644
2557.527022	140799.876073	57.747649
2557.259788	140653.445135	57.752653
2556.396869	140481.316581	57.757658
2555.832158	140349.012262	57.762663
2554.983215	140170.111129	57.767668
2554.638837	140028.612539	57.772673
2553.854533	139845.611900	57.777677
2552.932670	139715.920778	57.782682
2552.741237	139547.858552	57.787687
2551.532980	139387.378310	57.792692
2551.206250	139255.434971	57.797697
2550.351136	139065.297276	57.802701
2550.033613	138939.426949	57.807706
2549.438994	138758.041876	57.812711
2548.405919	138622.401769	57.817716
2548.219830	138431.247346	57.822721
2547.465735	138277.599881	57.827725
2546.523862	138132.647626	57.832730
2546.052204	137951.997579	57.837735
2545.058576	137801.668360	57.842740
2544.678817	137631.271054	57.847745
2543.621233	137488.423849	57.852749
2543.365349	137311.097518	57.857754
2542.626688	137156.005147	57.862759
2541.628397	137012.159921	57.867764
2540.899613	136854.628353	57.872769
2540.468879	136695.195592	57.877773
2539.665155	136535.517912	57.882778
2539.351069	136381.975771	57.887783
2538.445631	136208.811630	57.892788
2537.954590	136070.721757	57.897793
2537.180713	135888.988957	57.902797
2536.644142	135751.098372	57.907802
2536.205162	135596.055715	57.912807
2535.344637	135432.429537	57.917812
2534.692254	135262.394126	57.922817
2534.136975	135097.832215	57.927821
2533.342579	134944.729479	57.932826
2532.907905	134786.311371	57.937831
2532.067038	134616.703430	57.942836
2531.473476	134450.131461	57.947841
2530.544020	134291.565828	57.952845
2529.827848	134132.548068	57.957850
2529.105374	133983.084815	57.962855
2528.455577	133824.820417	57.967860
2528.155392	133654.649754	57.972865
2527.312107	133510.022482	57.977869
2526.455351	133349.545124	57.982874
2525.990467	133188.790618	57.987879
2525.298411	133034.551316	57.992884
2524.905638	132862.100884	57.997889
2524.260301	132714.003908	58.002893
2523.580682	132547.189902	58.007898
2523.047991	132373.507076	58.012903
2521.980299	132218.760130	58.017908
2521.176328	132060.911027	58.022913
2520.586715	131904.705499	58.027917
2520.014690	131747.494591	58.032922
2519.595693	131577.291672	58.037927
2518.879777	131426.748444	58.042932
2518.573059	131259.019207	58.047937
2517.730326	131098.031597	58.052941
2516.951491	130937.161798	58.057946
2516.366484	130771.511830	58.062951
2515.347762	130600.190522	58.067956
2515.055463	130440.021252	58.072961
2514.154440	130287.354235	58.077965
2513.625124	130127.389436	58.082970
2513.094129	129963.094722	58.087975
2512.238078	129803.590000	58.092980
2511.925242	129627.031544	58.097985
2511.143723	129474.667561	58.102989
2510.033856	129300.828489	58.107994
2509.725555	129148.048374	58.112999
2508.759225	129000.606088	58.118004
2508.317807	128824.428732	58.123009
2507.438209	128661.263818	58.128013
2506.866947	128505.506189	58.133018
2506.604147	128334.447345	58.138023
2505.393689	128180.532814	58.143028
2504.971635	128033.187233	58.148033
2504.478873	127866.676337	58.153037
2503.883905	127688.714439	58.158042
2502.855751	127523.725591	58.163047
2502.272615	127372.865768	58.168052
2501.773253	127206.372623	58.173057
2500.839675	127041.917782	58.178061
2500.121182	126887.335643	58.183066
2499.866391	126725.429370	58.188071
2498.835434	126569.120602	58.193076
2498.489478	126394.670841	58.198081
2497.813900	126242.612758	58.203085
2497.004366	126069.698992	58.208090
2496.729143	125913.756785	58.213095
2495.839000	125751.703019	58.218100
2495.558736	125580.270486	58.223105
2494.799741	125415.835904	58.228109
2494.009964	125244.905321	58.233114
2493.436681	125064.810999	58.238119
2492.375398	124916.402584	58.243124
2491.861894	124742.650353	58.248129
2491.495711	124576.380801	58.253133
2490.680122	124417.713771	58.258138
2490.141684	124250.495746	58.263143
2489.447205	124080.890794	58.268148
2488.871389	123908.423676	58.273153
2488.022170	123738.223200	58.278157
2487.075863	123571.975635	58.283162
2486.828974	123395.028025	58.288167
2485.863419	123246.080366	58.293172
2485.286410	123064.196948	58.298177
2484.467747	122895.254104	58.303181
2483.961742	122737.081294	58.308186
2483.340551	122567.144204	58.313191
2482.827300	122395.578495	58.318196
2482.316517	122220.902606	58.323201
2481.355700	122057.333298	58.328205
2480.611114	121890.594474	58.333210
2479.818371	121723.064405	58.338215
2479.151317	121570.142685	58.343220
2478.810143	121392.309175	58.348225
2478.240611	121224.162828	58.353229
2477.254953	121067.028317	58.358234
2476.991941	120893.299615	58.363239
2475.777872	120730.324658	58.368244
2475.595881	120560.115037	58.373249
2474.631897	120409.557946	58.378253
2474.297104	120219.580655	58.383258
2473.798888	120059.683251	58.388263
2472.853399	119898.004043	58.393268
2472.349228	119722.137556	58.398273
2471.676562	119543.410566	58.403277
2470.778689	119384.621745	58.408282
2470.128020	119198.834567	58.413287
2469.196202	119038.364665	58.418292
2468.770477	118896.808649	58.423297
2468.480917	118715.214486	58.428301
2467.509600	118543.981487	58.433306
2466.928126	118379.645061	58.438311
2465.981458	118208.588119	58.443316
2465.213472	118039.960571	58.448321
2464.463396	117889.206460	58.453325
2464.105678	117710.270822	58.458330
2463.451478	117548.020571	58.463335
2462.496386	117375.396291	58.468340
2462.423054	117220.609672	58.473345
2461.482760	117051.203439	58.478349
2461.040033	116887.330623	58.483354
2460.416245	116702.782244	58.488359
2459.350094	116557.214789	58.493364
2459.052857	116374.172133	58.498369
2458.560218	116211.561992	58.503373
2457.417773	116036.615258	58.508378
2456.757851	115860.596729	58.513383
2456.025173	115709.820976	58.518388
2455.769604	115538.037628	58.523393
2454.797834	115380.783223	58.528397
2453.998293	115215.086298	58.533402
2453.839718	115031.974208	58.538407
2453.097963	114876.857152	58.543412
2452.529963	114697.227059	58.548417
2451.805579	114528.926829	58.553421
2451.057761	114360.517195	58.558426
2450.633069	114178.138944	58.563431
2449.953956	114024.388116	58.568436
2449.225916	113834.780716	58.573441
2448.678357	113671.084950	58.578445
2447.815209	113498.085357	58.583450
2447.384290	113322.663864	58.588455
2446.457435	113163.087009	58.593460
2446.026847	112994.046040	58.598465
2445.243090	112812.654891	58.603469
2444.687544	112639.219007	58.608474
2444.110700	112458.686132	58.613479
2443.204467	112299.777906	58.618484
2442.842508	112123.014850	58.623489
2442.018551	111945.076081	58.628493
2441.279152	111765.887680	58.633498
2440.734062	111596.639554	58.638503
2439.809136	111430.473540	58.643508
2439.238821	111252.588389	58.648513
2438.555483	111080.351341	58.653517
2437.804892	110906.907734	58.658522
2437.088499	110755.397768	58.663527
2436.401079	110554.995513	58.668532
2436.137936	110397.901338	58.673537
2435.410588	110239.885467	58.678541
2434.647524	110053.504455	58.683546
2434.318317	109883.408937	58.688551
2433.381203	109709.546467	58.693556
2432.931823	109527.821859	58.698561
2432.065567	109356.596785	58.703565
2431.705868	109188.973011	58.708570
2431.181120	109006.477388	58.713575
2429.985510	108826.272307	58.718580
2429.662076	108640.581151	58.723585
2428.515308	108462.629978	58.728589
2427.780327	108307.508613	58.733594
2427.423359	108128.273503	58.738599
2426.704437	107961.952460	58.743604
2426.254272	107776.465676	58.748609
2425.382006	107616.300734	58.753613
2424.770852	107431.679673	58.758618
2424.595128	107260.905603	58.763623
2423.359495	107094.583620	58.768628
2422.995855	106908.613921	58.773633
2422.179667	106740.375180	58.778637
2421.472321	106555.319260	58.783642
2420.729582	106386.405150	58.788647
2420.214895	106204.373237	58.793652
2419.547059	106024.454387	58.798657
2418.994701	105857.645642	58.803661
2418.278807	105676.201630	58.808666
2417.735507	105503.176225	58.813671
2417.080750	105334.706065	58.818676
2416.313376	105145.058129	58.823681
2415.726280	104960.306381	58.828685
2414.627786	104793.775653	58.833690
2414.433653	104627.813288	58.838695
2413.337434	104454.730906	58.843700
2413.117586	104274.627379	58.848705
2412.056311	104099.226418	58.853709
2411.403224	103929.528859	58.858714
2410.909293	103756.730408	58.863719
2409.802478	103582.260401	58.868724
2409.428385	103398.464061	58.873729
2408.871887	103229.263748	58.878733
2408.196185	103063.870853	58.883738
2407.763942	102884.471377	58.888743
2407.212726	102712.279655	58.893748
2406.226645	102527.369140	58.898753
2405.285668	102358.470778	58.903757
2404.628296	102202.824981	58.908762
2404.264666	101998.833398	58.913767
2403.603579	101845.702637	58.918772
2403.053291	101674.013211	58.923777
2402.224228	101498.645629	58.928781
2401.191573	101326.267681	58.933786
2401.195615	101151.836329	58.938791
2400.285982	100976.745536	58.943796
2400.029255	100803.220836	58.948801
2399.317122	100622.519321	58.953805
2398.593556	100442.905713	58.958810
2398.073644	100262.715702	58.963815
2397.038309	100090.708928	58.968820
2396.360640	99905.922604	58.973825
2395.986497	99733.528231	58.978829
2394.971870	99555.788107	58.983834
2394.624822	99376.706654	58.988839
2393.851598	99201.791636	58.993844
2392.978722	99024.198063	58.998849
2392.177153	98846.645302	59.003853
2391.209751	98682.985336	59.008858
2391.038490	98507.441049	59.013863
2390.159942	98331.604316	59.018868
2389.605094	98152.565369	59.023873
2389.129368	97977.333466	59.028877
2388.666419	97811.481371	59.033882
2388.199526	97638.489557	59.038887
2387.210082	97467.053333	59.043892
2386.946496	97276.495426	59.048897
2385.985630	97096.755389	59.053901
2385.230445	96922.711178	59.058906
2385.196890	96727.187175	59.063911
2383.943029	96556.028075	59.068916
2383.345212	96370.312719	59.073921
2382.740053	96192.603657	59.078925
2382.257291	96016.214740	59.083930
2381.475305	95837.845234	59.088935
2380.693803	95656.876905	59.093940
2380.198136	95468.825317	59.098945
2379.361871	95292.142977	59.103949
2378.453993	95119.665244	59.108954
2377.797765	94930.058198	59.113959
2377.132328	94762.529308	59.118964
2376.561232	94591.353005	59.123969
2375.936421	94410.376228	59.128973
2375.303275	94234.538811	59.133978
2374.931336	94057.056990	59.138983
2373.942315	93886.408931	59.143988
2373.333569	93705.473371	59.148993
2372.472558	93523.894423	59.153997
2371.675058	93341.032309	59.159002
2371.368192	93162.412227	59.164007
2370.497575	92985.417511	59.169012
2369.843076	92817.001078	59.174017
2369.468608	92649.004420	59.179021
2368.951272	92460.144614	59.184026
2368.026438	92282.885109	59.189031
2367.068162	92113.837379	59.194036
2366.672397	91925.038963	59.199041
2366.096580	91752.984893	59.204045
2365.445645	91579.834457	59.209050
2364.794133	91386.953414	59.214055
2364.147975	91225.313266	59.219060
2363.662881	91048.222240	59.224065
2362.882436	90855.233159	59.229069
2361.990760	90675.901672	59.234074
2361.384633	90496.101574	59.239079
2360.721176	90325.106075	59.244084
2360.116988	90141.130315	59.249089
2359.525442	89970.481247	59.254093
2358.719773	89797.020726	59.259098
2358.219879	89612.417893	59.264103
2357.598760	89437.257186	59.269108
2356.910276	89249.885020	59.274113
2355.870575	89073.836270	59.279117
2355.446797	88892.581322	59.284122
2354.924261	88716.707068	59.289127
2353.979456	88544.907954	59.294132
2353.707891	88352.234420	59.299137
2353.108579	88184.041429	59.304141
2352.456130	88010.184185	59.309146
2351.654186	87814.924208	59.314151
2350.725252	87639.104145	59.319156
2350.158668	87452.571383	59.324161
2349.442545	87275.928109	59.329165
2348.450499	87106.461846	59.334170
2348.359083	86923.744374	59.339175
2347.726758	86752.537606	59.344180
2346.989685	86568.321701	59.349185
2346.316266	86393.200341	59.354189
2345.632813	86221.422724	59.359194
2345.059360	86038.472282	59.364199
2344.415287	85850.127426	59.369204
2343.824994	85665.851656	59.374209
2343.044632	85490.444051	59.379213
2342.260528	85305.726711	59.384218
2341.678143	85127.596696	59.389223
2340.966321	84950.769125	59.394228
2340.376291	84761.753429	59.399233
2339.769205	84584.848915	59.404237
2338.374215	84404.749395	59.409242
2338.270244	84231.089478	59.414247
2337.495082	84054.108297	59.419252
2337.145787	83870.019084	59.424257
2336.464684	83696.645225	59.429261
2335.662673	83511.661155	59.434266
2335.481100	83333.831298	59.439271
2334.527254	83157.253601	59.444276
2333.881597	82984.520146	59.449281
2333.342136	82777.640615	59.454285
2332.338057	82596.657949	59.459290
2332.365411	82403.857746	59.464295
2331.215473	82252.829144	59.469300
2330.809461	82047.944782	59.474305
2329.989814	81862.274551	59.479309
2329.136013	81684.032905	59.484314
2328.887558	81499.549219	59.489319
2327.971276	81309.849436	59.494324
2327.060059	81123.724982	59.499329
2326.713977	80954.807720	59.504333
2325.599262	80773.598578	59.509338
2325.315153	80586.961218	59.514343
2324.324088	80416.338110	59.519348
2323.980624	80227.862881	59.524353
2323.096228	80056.091448	59.529357
2322.395287	79862.967641	59.534362
2322.116735	79676.667141	59.539367
2321.273900	79498.138358	59.544372
2320.654430	79315.196808	59.549377
2320.174866	79135.669342	59.554381
2319.366178	78957.868581	59.559386
2318.763048	78768.915552	59.564391
2317.698781	78588.180191	59.569396
2317.010768	78401.119705	59.574401
2316.601688	78230.321026	59.579405
2315.939798	78053.011765	59.584410
2315.400459	77856.085531	59.589415
2314.612690	77688.469026	59.594420
2313.957596	77500.258306	59.599425
2313.394094	77316.235844	59.604429
2312.750372	77142.644747	59.609434
2312.206289	76952.932429	59.614439
2311.268678	76768.296258	59.619444
2310.608959	76590.245355	59.624449
2310.357942	76404.109652	59.629453
2309.151844	76223.024900	59.634458
2308.747380	76036.543074	59.639463
2307.814032	75855.481717	59.644468
2307.611360	75666.025080	59.649473
2306.661937	75495.601146	59.654477
2306.096982	75303.854754	59.659482
2305.589015	75121.902526	59.664487
2304.810686	74941.965209	59.669492
2304.169738	74752.390244	59.674497
2303.573940	74566.199429	59.679501
2302.983536	74383.075866	59.684506
2302.293613	74202.180825	59.689511
2301.062796	74011.863775	59.694516
2300.573071	73823.534339	59.699521
2300.129766	73647.895189	59.704525
2299.631153	73466.171876	59.709530
2299.005828	73284.185227	59.714535
2298.049782	73092.699359	59.719540
2297.285302	72912.461313	59.724545
2296.656820	72732.158986	59.729549
2295.766365	72558.671868	59.734554
2295.532229	72370.746379	59.739559
2295.002220	72201.050483	59.744564
2294.441415	72013.104162	59.749569
2293.620167	71824.668808	59.754573
2293.066502	71633.405574	59.759578
2291.983892	71450.881092	59.764583
2291.125261	71281.663264	59.769588
2290.927508	71093.560406	59.774593
2290.142907	70903.316362	59.779597
2289.616370	70729.027428	59.784602
2288.972700	70537.478692	59.789607
2288.420889	70358.427333	59.794612
2287.551327	70185.217420	59.799617
2287.133298	69984.479083	59.804621
2286.170726	69801.792487	59.809626
2285.537989	69626.168348	59.814631
2284.817788	69442.015186	59.819636
2284.368435	69253.805132	59.824641
2283.422241	69076.297472	59.829645
2282.605496	68893.026186	59.834650
2282.249772	68698.403210	59.839655
2281.390595	68525.136663	59.844660
2280.993894	68347.048133	59.849665
2280.373511	68165.234599	59.854669
2279.590975	67979.471071	59.859674
2279.304888	67793.567251	59.864679
2278.281510	67615.743134	59.869684
2277.616820	67424.323227	59.874689
2277.125925	67235.448928	59.879693
2276.138780	67056.427220	59.884698
2275.736551	66873.641212	59.889703
2274.824422	66687.071482	59.894708
2274.279531	66511.382352	59.899713
2274.068120	66328.438244	59.904718
2273.076279	66144.717210	59.909722
2272.518867	65948.697249	59.914727
2271.766875	65769.789502	59.919732
2271.125547	65586.097370	59.924737
2270.572675	65396.319995	59.929742
2269.713304	65220.993312	59.934746
2269.189739	65021.770000	59.939751
2268.581999	64844.624257	59.944756
2267.743807	64659.699400	59.949761
2267.275744	64474.372518	59.954766
2266.805926	64285.469997	59.959770
2266.075745	64086.058068	59.964775
2265.324478	63914.857954	59.969780
2264.720824	63720.948215	59.974785
2264.063888	63536.635530	59.979790
2263.084684	63353.249548	59.984794
2262.748150	63153.382875	59.989799
2261.722180	62969.112060	59.994804
2261.193346	62779.809604	59.999809
2260.372673	62612.732025	60.004814
2259.544100	62413.331087	60.009818
2259.651064	62241.649036	60.014823
2258.638969	62050.752651	60.019828
2257.699009	61866.013568	60.024833
2257.261861	61679.471250	60.029838
2256.544592	61496.789816	60.034842
2256.157557	61306.710368	60.039847
2255.544431	61111.011788	60.044852
2254.827353	60931.178512	60.049857
2253.991198	60743.955341	60.054862
2253.377577	60555.267940	60.059866
2252.763422	60366.769284	60.064871
2252.026179	60179.456924	60.069876
2251.019597	59988.425496	60.074881
2250.893441	59801.197264	60.079886
2249.817720	59625.089404	60.084890
2249.136784	59439.222089	60.089895
2248.433983	59254.046958	60.094900
2247.924161	59054.764060	60.099905
2247.502527	58876.606575	60.104910
2246.592674	58700.680552	60.109914
2246.352636	58520.671363	60.114919
2245.558383	58333.079569	60.119924
2244.948291	58124.146781	60.124929
2244.400553	57935.548228	60.129934
2243.688860	57745.176703	60.134938
2242.964711	57568.070408	60.139943
2242.217088	57377.872941	60.144948
2241.629526	57167.279447	60.149953
2240.881338	56979.200342	60.154958
2239.962867	56800.818797	60.159962
2239.475583	56623.608038	60.164967
2238.934822	56421.987918	60.169972
2238.251032	56231.197175	60.174977
2237.732449	56036.537069	60.179982
2236.643808	55861.486106	60.184986
2236.016990	55662.381751	60.189991
2234.991625	55478.200698	60.194996
2234.624185	55304.113480	60.200001
2233.821058	55103.897576	60.205006
2233.438037	54930.965116	60.210010
2232.965620	54739.387399	60.215015
2232.148277	54556.366165	60.220020
2231.548817	54374.495709	60.225025
2230.924049	54179.821570	60.230030
2230.046028	54006.409961	60.235034
2229.908466	53807.207093	60.240039
2228.663359	53628.538061	60.245044
2228.316187	53427.521482	60.250049
2227.541524	53236.032845	60.255054
2226.867749	53070.733040	60.260058
2226.094332	52873.005057	60.265063
2225.344120	52675.060391	60.270068
2224.749182	52507.611104	60.275073
2224.431387	52313.886015	60.280078
2223.740657	52130.014879	60.285082
2223.340866	51930.152846	60.290087
2222.673445	51755.267629	60.295092
2221.811897	51550.139093	60.300097
2221.191466	51347.113455	60.305102
2220.062707	51178.824674	60.310106
2220.069280	50989.580402	60.315111
2219.295282	50780.333772	60.320116
2218.584766	50602.790031	60.325121
2217.807129	50415.292900	60.330126
2217.134219	50211.975228	60.335130
2216.596895	50019.682746	60.340135
2215.506409	49832.149610	60.345140
2215.178317	49630.375176	60.350145
2214.338733	49448.823453	60.355150
2213.720913	49257.507355	60.360154
2213.134419	49051.168028	60.365159
2212.378139	48886.264680	60.370164
2211.912004	48697.179779	60.375169
2211.261440	48496.864425	60.380174
2210.353835	48324.236802	60.385178
2209.860274	48116.840190	60.390183
2209.206087	47932.639503	60.395188
2208.427456	47737.398522	60.400193
2208.075079	47551.875967	60.405198
2206.864683	47363.401014	60.410202
2206.644401	47166.110270	60.415207
2206.149858	46980.815548	60.420212
2205.390752	46781.599662	60.425217
2204.423502	46612.721201	60.430222
2203.901984	46384.735686	60.435226
2203.516082	46212.612154	60.440231
2202.427698	46032.074393	60.445236
2201.894393	45830.072214	60.450241
2201.386045	45642.029403	60.455246
2200.204268	45448.974769	60.460250
2199.881826	45253.695329	60.465255
2199.241414	45084.893607	60.470260
2198.548180	44883.244007	60.475265
2197.924783	44699.900970	60.480270
2197.149135	44513.367559	60.485274
2196.231783	44323.879404	60.490279
2195.688703	44130.504012	60.495284
2195.198503	43951.186393	60.500289
2194.457209	43753.169177	60.505294
2193.531987	43570.028240	60.510298
2193.029337	43393.374870	60.515303
2192.470517	43195.809443	60.520308
2192.060675	42995.170911	60.525313
2191.076094	42819.678223	60.530318
2190.636138	42622.891076	60.535322
2190.353180	42427.713016	60.540327
2189.522551	42247.859870	60.545332
2188.821817	42072.642815	60.550337
2188.186780	41863.372800	60.555342
2187.205257	41668.956070	60.560346
2186.514254	41484.007150	60.565351
2186.205175	41293.503906	60.570356
2185.292070	41100.844040	60.575361
2184.772170	40907.984834	60.580366
2184.170200	40721.616577	60.585370
2183.673925	40526.647283	60.590375
2182.477539	40337.933305	60.595380
2182.141209	40146.960189	60.600385
2181.885172	39946.582607	60.605390
2180.937668	39768.059291	60.610394
2180.169930	39572.849893	60.615399
2179.626847	39374.625567	60.620404
2178.664116	39175.553224	60.625409
2177.803242	38984.918201	60.630414
2176.993471	38815.392214	60.635418
2177.005858	38604.930655	60.640423
2175.871831	38424.734278	60.645428
2175.145001	38244.922578	60.650433
2174.565690	38058.605148	60.655438
2174.199423	37867.516935	60.660442
2173.483734	37668.971597	60.665447
2172.823467	37483.112785	60.670452
2172.176486	37293.341730	60.675457
2171.587388	37095.067579	60.680462
2170.945523	36915.017868	60.685466
2170.230203	36717.819306	60.690471
2169.315324	36538.031902	60.695476
2168.410105	36335.514430	60.700481
2168.049464	36144.669287	60.705486
2167.291762	35971.186878	60.710490
2167.008990	35772.105252	60.715495
2166.073090	35596.775729	60.720500
2165.561858	35397.799594	60.725505
2164.906485	35202.733513	60.730510
2164.001649	35012.787312	60.735514
2163.727787	34828.281055	60.740519
2162.885261	34635.596668	60.745524
2162.184576	34447.484676	60.750529
2161.777330	34254.342118	60.755534
2160.902684	34066.702952	60.760538
2160.306887	33869.327762	60.765543
2159.574795	33688.303003	60.770548
2158.978158	33494.706242	60.775553
2158.017671	33304.363251	60.780558
2157.634989	33123.908693	60.785562
2156.946723	32917.657745	60.790567
2156.373007	32730.505851	60.795572
2155.089889	32545.846861	60.800577
2154.926062	32350.532404	60.805582
2154.027775	32167.625931	60.810586
2153.406257	31984.345741	60.815591
2152.777857	31784.067766	60.820596
2151.949146	31603.003721	60.825601
2151.302290	31429.456321	60.830606
2150.449269	31234.120630	60.835610
2150.228388	31032.374534	60.840615
2149.539539	30873.842568	60.845620
2148.992688	30649.791761	60.850625
2148.228564	30517.420249	60.855630
2147.266862	30319.712609	60.860634
2146.764951	30113.622050	60.865639
2146.208305	29906.305648	60.870644
2145.479279	29724.526049	60.875649
2144.899867	29587.250689	60.880654
2143.911321	29397.221198	60.885658
2143.550331	29180.871062	60.890663
2142.839337	29017.928962	60.895668
2141.889111	28819.739995	60.900673
2141.602514	28645.288133	60.905678
2140.250578	28451.701564	60.910682
2140.333683	28269.425453	60.915687
2139.230732	28082.617536	60.920692
2138.905172	27912.356713	60.925697
2137.994133	27728.403954	60.930702
2137.409898	27528.057384	60.935706
2136.779991	27352.656526	60.940711
2136.316401	27169.626457	60.945716
2135.159089	26979.842391	60.950721
2134.317894	26812.915679	60.955726
2133.781747	26615.167411	60.960730
2133.292548	26472.206274	60.965735
2132.523350	26259.173668	60.970740
2131.547606	26111.630675	60.975745
2131.642521	25906.478194	60.980750
2130.466762	25734.745874	60.985754
2129.715129	25563.699177	60.990759
2129.518511	25359.567405	60.995764
2128.645469	25206.053702	61.000769
2128.450847	25013.238527	61.005774
2127.389202	24815.140089	61.010778
2126.760593	24657.811588	61.015783
2125.533680	24462.687858	61.020788
2125.199220	24284.793072	61.025793
2124.686485	24135.170781	61.030798
2123.683197	23931.607696	61.035802
2123.302080	23761.462007	61.040807
2122.735288	23579.072827	61.045812
2121.873911	23412.330032	61.050817
2121.146062	23220.297849	61.055822
2120.621421	23040.130263	61.060826
2119.978937	22884.563435	61.065831
2119.340970	22681.646949	61.070836
2118.461087	22526.780639	61.075841
2118.023114	22336.233185	61.080846
2116.910482	22195.597249	61.085850
2116.126402	21991.586008	61.090855
2115.528109	21840.780542	61.095860
2114.824336	21653.471853	61.100865
2114.307525	21498.884885	61.105870
2113.372489	21327.923850	61.110874
2113.312512	21146.183381	61.115879
2112.230473	20994.789257	61.120884
2111.141740	20827.999220	61.125889
2110.827059	20646.393355	61.130894
2109.766298	20493.333583	61.135898
2109.204330	20330.547874	61.140903
2108.473286	20182.128942	61.145908
2107.801289	20019.040615	61.150913
2107.375728	19846.531371	61.155918
2106.296867	19685.421640	61.160922
2105.939777	19543.169766	61.165927
2105.258429	19376.199463	61.170932
2104.225520	19215.295700	61.175937
2104.020382	19063.438450	61.180942
2102.832848	18919.959043	61.185946
2102.243472	18729.580727	61.190951
2101.351974	18610.591296	61.195956
2100.681994	18445.759409	61.200961
2100.188607	18292.557326	61.205966
2099.197256	18169.087059	61.210970
2098.624736	18001.810267	61.215975
2097.846315	17857.980096	61.220980
2096.659916	17708.513084	61.225985
2096.422236	17566.106352	61.230990
2095.847566	17437.007522	61.235994
2094.929763	17281.298542	61.240999
2094.130825	17163.607551	61.246004
2093.318925	17025.682159	61.251009
2092.415909	16880.627328	61.256014
2091.526445	16752.437426	61.261018
2091.061951	16634.660288	61.266023
2089.878038	16529.511940	61.271028
2089.083649	16394.386958	61.276033
2088.478336	16246.967280	61.281038
2087.552135	16164.514634	61.286042
2087.067876	16037.453482	61.291047
2086.189407	15938.776357	61.296052
2085.567185	15836.940725	61.301057
2084.742113	15712.831733	61.306062
2083.773841	15621.885829	61.311066
2083.379841	15508.261348	61.316071
2082.334824	15407.745750	61.321076
2081.662713	15315.481181	61.326081
2080.847943	15230.014000	61.331086
2079.653245	15138.861523	61.336090
2078.714306	15061.477796	61.341095
2077.698785	14966.798874	61.346100
2077.171110	14858.229669	61.351105
2076.394413	14812.942999	61.356110
2075.565901	14764.547015	61.361114
2074.656553	14669.166352	61.366119
2074.300453	14578.541269	61.371124
2073.363776	14563.834777	61.376129
2073.020090	14464.376227	61.381134
2072.328787	14395.660563	61.386138
2071.441386	14348.057254	61.391143
2070.859439	14246.996140	61.396148
2070.542062	14218.588451	61.401153
2070.029398	14139.661190	61.406158
2069.185610	14072.729611	61.411162
2068.737252	13989.832329	61.416167
2067.912453	13930.278807	61.421172
2066.767524	13866.079960	61.426177
2066.649783	13785.042538	61.431182
2065.742703	13716.228823	61.436186
2065.108166	13671.839611	61.441191
2064.433075	13602.923969	61.446196
2064.125759	13543.099650	61.451201
2063.443116	13485.010626	61.456206
2062.356835	13430.446462	61.461210
2062.292451	13346.449449	61.466215
2061.514581	13283.761984	61.471220
2060.492258	13223.896717	61.476225
2060.110567	13134.734025	61.481230
2059.271971	13106.137381	61.486234
2058.867697	13010.702904	61.491239
2058.156710	12976.913815	61.496244
2057.680126	12886.383479	61.501249
2057.253611	12821.541282	61.506254
2056.301604	12738.042697	61.511258
2055.567010	12700.173636	61.516263
2055.333776	12615.977114	61.521268
2054.505768	12559.548865	61.526273
2054.130225	12478.543411	61.531278
2053.121676	12422.816450	61.536282
2052.408261	12353.508052	61.541287
2051.588538	12287.669967	61.546292
2051.106911	12216.657242	61.551297
2050.468291	12142.433669	61.556302
2049.789491	12084.241182	61.561306
2049.051590	12014.060943	61.566311
2048.639031	11954.282058	61.571316
2047.617882	11884.072408	61.576321
2046.831947	11831.872252	61.581326
2046.108941	11765.935667	61.586330
2045.643245	11702.588130	61.591335
2045.170115	11643.653346	61.596340
2044.355075	11582.626782	61.601345
2044.061070	11519.530319	61.606350
2042.950389	11454.840013	61.611354
2042.502939	11385.666640	61.616359
2041.989912	11327.400847	61.621364
2041.257003	11267.168740	61.626369
2040.975529	11195.687166	61.631374
2039.954032	11134.194722	61.636378
2039.477639	11066.533689	61.641383
2038.955382	11004.831170	61.646388
2037.905342	10937.401805	61.651393
2037.162067	10876.091925	61.656398
2036.646929	10810.469158	61.661402
2035.906874	10734.950316	61.666407
2035.328363	10670.054257	61.671412
2034.360720	10620.462887	61.676417
2033.893178	10545.029768	61.681422
2033.237161	10485.465554	61.686426
2032.735391	10438.852749	61.691431
2032.055988	10367.393271	61.696436
2031.384813	10302.780182	61.701441
2030.855997	10239.855329	61.706446
2029.888168	10194.334658	61.711450
2029.253122	10125.448125	61.716455
2028.668849	10065.591728	61.721460
2027.969315	9991.656644	61.726465
2027.467616	9917.563501	61.731470
2026.544172	9873.965031	61.736474
2026.034872	9810.776144	61.741479
2025.126226	9747.885619	61.746484
2024.580530	9704.348801	61.751489
2024.265617	9630.031767	61.756494
2023.746230	9562.832442	61.761498
2022.957386	9499.690411	61.766503
2022.047021	9454.387721	61.771508
2021.458334	9377.602947	61.776513
2020.596488	9327.310698	61.781518
2019.926857	9269.792508	61.786522
2019.663712	9205.497288	61.791527
2019.194756	9144.748559	61.796532
2018.443723	9084.150560	61.801537
2017.691455	9016.086913	61.806542
2016.827044	8949.790435	61.811546
2016.057751	8886.362687	61.816551
2015.566804	8832.797566	61.821556
2015.112202	8766.515753	61.826561
2014.168739	8701.069180	61.831566
2013.587300	8656.332851	61.836570
2012.860520	8588.307735	61.841575
2012.289662	8520.073183	61.846580
2011.321625	8467.603962	61.851585
2010.934530	8394.969488	61.856590
2009.939481	8347.944852	61.861594
2009.381482	8281.422051	61.866599
2008.603930	8237.426530	61.871604
2007.714647	8174.032682	61.876609
2007.115408	8118.321803	61.881614
2006.947453	8065.530979	61.886618
2006.336627	8004.962042	61.891623
2005.981309	7947.102831	61.896628
2005.203604	7890.292241	61.901633
2004.914824	7820.051818	61.906638
2003.810493	7759.951903	61.911642
2002.865947	7698.140276	61.916647
2002.259900	7636.589151	61.921652
2001.794158	7577.297392	61.926657
2001.027390	7508.313643	61.931662
1999.898408	7468.799677	61.936666
1999.490397	7397.400043	61.941671
1999.182944	7354.227868	61.946676
1998.210699	7295.827764	61.951681
1997.945085	7227.253284	61.956686
1997.095923	7172.925057	61.961690
1996.758047	7118.569522	61.966695
1996.114993	7050.241138	61.971700
1995.315046	6983.009985	61.976705
1994.648337	6919.398415	61.981710
1993.814188	6871.000870	61.986714
1993.423722	6794.219214	61.991719
1992.521496	6737.521139	61.996724
1991.427923	6674.356210	62.001729
1990.889182	6613.651341	62.006734
1989.932537	6569.069181	62.011738
1989.677813	6510.798871	62.016743
1988.922807	6457.105140	62.021748
1988.084958	6398.802402	62.026753
1987.847278	6340.865293	62.031758
1986.918390	6285.394234	62.036762
1986.329346	6223.725576	62.041767
1985.788032	6173.177772	62.046772
1984.909391	6120.051514	62.051777
1984.678821	6058.823580	62.056782
1983.869606	6000.140831	62.061786
1983.327193	5945.047478	62.066791
1982.396379	5885.072757	62.071796
1981.709909	5824.732159	62.076801
1980.917090	5766.140812	62.081806
1979.990687	5718.187612	62.086810
1979.575033	5657.224187	62.091815
1978.971112	5606.941446	62.096820
1978.245163	5555.391000	62.101825
1977.813062	5505.036375	62.106830
1977.320418	5458.628165	62.111834
1976.675104	5400.723939	62.116839
1975.917856	5337.467960	62.121844
1975.033464	5277.591664	62.126849
1974.813543	5221.426830	62.131854
1973.566945	5161.230693	62.136858
1972.804649	5104.407829	62.141863
1972.687591	5053.647445	62.146868
1972.186762	4990.408255	62.151873
1971.357815	4936.215963	62.156878
1970.608849	4880.383266	62.161882
1970.167776	4822.494637	62.166887
1969.550047	4763.317129	62.171892
1968.694553	4708.282816	62.176897
1968.243573	4637.400971	62.181902
1967.274631	4586.177205	62.186906
1966.303267	4535.523443	62.191911
1966.150569	4480.876098	62.196916
1965.266660	4419.746824	62.201921
1964.730199	4369.453652	62.206926
1964.045040	4311.006372	62.211930
1963.576612	4234.836367	62.216935
1962.869313	4188.779334	62.221940
1961.848942	4134.609339	62.226945
1961.447202	4066.976503	62.231950
1960.667528	4015.426569	62.236954
1960.009223	3963.015256	62.241959
1959.591531	3907.733058	62.246964
1958.542914	3847.843696	62.251969
1958.044465	3792.913083	62.256974
1957.211364	3739.549223	62.261978
1956.589681	3686.457997	62.266983
1956.344292	3632.207069	62.271988
1955.088396	3578.895920	62.276993
1954.871524	3519.414524	62.281998
1954.089621	3458.851925	62.287002
1953.421549	3406.973327	62.292007
1952.753167	3354.947488	62.297012
1952.089551	3295.082871	62.302017
1951.635865	3244.577737	62.307022
1950.568332	3187.923511	62.312026
1949.950816	3124.210882	62.317031
1949.231255	3067.588637	62.322036
1948.387889	3025.507052	62.327041
1947.966845	2966.648614	62.332046
1946.951336	2920.851897	62.337050
1946.393861	2870.146085	62.342055
1945.854675	2811.653222	62.347060
1945.159253	2785.716835	62.352065
1944.838342	2712.722795	62.357070
1944.264253	2664.173999	62.362074
1943.338984	2611.162464	62.367079
1943.090939	2561.600171	62.372084
1942.148889	2509.753263	62.377089
1941.817438	2449.628828	62.382094
1941.035853	2398.040737	62.387098
1940.014390	2330.225664	62.392103
1939.517908	2282.385793	62.397108
1938.588304	2227.280306	62.402113
1937.886251	2173.482631	62.407118
1937.067746	2126.208537	62.412122
1936.867524	2063.959383	62.417127
1936.348608	2014.652489	62.422132
1935.235958	1957.459001	62.427137
1934.666009	1908.927046	62.432142
1934.178598	1876.005773	62.437146
1933.679332	1821.837341	62.442151
1932.654123	1765.386950	62.447156
1931.746413	1707.682477	62.452161
1931.267212	1659.848214	62.457166
1930.778812	1616.620646	62.462170
1930.088941	1558.744189	62.467175
1929.291031	1515.193864	62.472180
1928.338518	1473.749937	62.477185
1927.889669	1416.047116	62.482190
1927.282536	1371.623211	62.487194
1926.673416	1320.257585	62.492199
1926.128710	1279.591623	62.497204
1925.289663	1225.591317	62.502209
1924.688588	1175.119109	62.507214
1923.980395	1134.473197	62.512218
1923.260993	1080.941739	62.517223
1922.622477	1028.089950	62.522228
1922.000361	992.713780	62.527233
1921.440262	945.527093	62.532238
1920.690821	891.477537	62.537242
1920.339551	842.178758	62.542247
1919.404884	792.464177	62.547252
1918.534023	763.082778	62.552257
1918.243047	700.230950	62.557262
1917.052085	658.617471	62.562266
1916.487366	613.485823	62.567271
1915.807423	572.422260	62.572276
1914.684334	525.709516	62.577281
1914.558633	481.919969	62.582286
1913.812086	444.081184	62.587290
1912.966483	394.533606	62.592295
1912.035129	356.680234	62.597300
1911.474562	323.338075	62.602305
1911.062599	282.026217	62.607310
1910.134567	243.516610	62.612314
1909.386600	201.644895	62.617319
1909.317700	162.656925	62.622324
1908.160660	120.796768	62.627329
1907.495985	85.913688	62.632334
1906.994505	63.885003	62.637338
1906.476087	23.962697	62.642343
1905.560406	-8.943863	62.647348
1904.527300	-50.607159	62.652353
1904.041602	-82.217792	62.657358
1902.977233	-102.630427	62.662362
1901.486500	-109.243764	62.667367
1896.189557	-7.566429	62.672372
1896.182955	12.139673	62.677377
1897.174905	-0.800164	62.682382
1897.380124	-0.867396	62.687386
1897.728804	-4.248404	62.692391
1897.733694	-3.198923	62.697396
1896.465979	-1.669878	62.702401
1895.741833	0.750557	62.707406
1894.808730	10.527317	62.712410
1894.130039	7.555401	62.717415
1893.180985	1.693362	62.722420
1892.313360	10.598737	62.727425
1892.379151	0.884051	62.732430
1891.674636	6.570297	62.737434
1890.789278	18.089849	62.742439
1890.194628	17.233416	62.747444
1890.157855	12.964297	62.752449
1889.735545	4.853543	62.757454
1888.284080	12.374046	62.762458
1887.914130	13.290654	62.767463
1887.541117	15.116046	62.772468
1886.546679	17.109477	62.777473
1885.877349	23.036142	62.782478
1885.317221	26.524918	62.787482
1884.493454	25.668590	62.792487
1883.950543	14.900965	62.797492
1883.142254	18.604173	62.802497
1882.452599	8.064848	62.807502
1881.609817	15.513955	62.812506
1880.745242	20.525471	62.817511
1880.643170	21.872625	62.822516
1880.461560	29.875920	62.827521
1879.535589	22.154193	62.832526
1878.353535	27.283922	62.837530
1877.938340	29.598548	62.842535
1878.100329	23.440274	62.847540
1876.870545	32.467815	62.852545
1875.644350	25.497052	62.857550
1874.930415	23.183574	62.862554
1875.211143	20.645953	62.867559
1874.751718	21.554691	62.872564
1873.098693	35.452691	62.877569
1872.907411	25.772495	62.882574
1872.205430	24.032691	62.887578
1871.553806	23.764032	62.892583
1870.893197	19.073575	62.897588
1870.006071	29.734007	62.902593
1869.613314	19.865035	62.907598
1869.205976	25.245499	62.912602
1868.037633	28.394037	62.917607
1867.485523	20.461577	62.922612
1866.994580	33.080709	62.927617
1866.477368	23.292994	62.932622
1865.314264	32.223223	62.937626
1864.919391	31.178963	62.942631
1864.640820	21.887934	62.947636
1862.985414	25.263608	62.952641
1862.825547	19.017667	62.957646
1862.554513	31.284925	62.962650
1862.200580	22.964621	62.967655
1861.162817	8.757493	62.972660
1859.584794	36.159258	62.977665
1859.491411	20.010816	62.982670
1859.258926	27.377232	62.987674
1858.476616	28.012393	62.992679
1857.336549	22.043496	62.997684
1857.234279	20.607441	63.002689
1856.597512	16.594427	63.007694
1855.530635	22.301948	63.012698
1855.089541	22.282134	63.017703
1854.487194	11.542880	63.022708
1853.336597	25.310649	63.027713
1853.053316	17.592550	63.032718
1852.528130	22.454000	63.037722
1852.050439	23.780369	63.042727
1851.398152	21.546994	63.047732
1850.996501	24.610080	63.052737
1850.429114	20.644397	63.057742
1849.609503	25.618824	63.062746
1848.614402	17.203211	63.067751
1847.671829	16.914522	63.072756
1846.994894	21.579299	63.077761
1846.350445	11.860683	63.082766
1845.641953	22.674098	63.087770
1845.538792	20.112273	63.092775
1844.919000	19.695068	63.097780
1844.185473	21.800050	63.102785
1843.190279	4.252596	63.107790
1842.746821	27.155070	63.112794
1842.306472	21.090855	63.117799
1841.794663	18.182340	63.122804
1840.353473	14.610856	63.127809
1839.848543	11.242371	63.132814
1839.520602	10.277373	63.137818
1838.292649	14.550257	63.142823
1837.894447	11.201096	63.147828
1836.859302	18.800601	63.152833
1837.123508	18.168928	63.157838
1835.997987	21.521984	63.162842
1835.355578	14.387597	63.167847
1834.969670	15.434475	63.172852
1834.272694	16.970700	63.177857
1833.787698	18.263539	63.182862
1833.407850	23.196530	63.187866
1832.132446	25.431705	63.192871
1831.436630	15.279715	63.197876
1830.499394	26.359682	63.202881
1830.326730	19.660051	63.207886
1829.714961	7.810585	63.212890
1828.966297	15.553834	63.217895
1828.540690	17.695081	63.222900
1827.647295	22.083580	63.227905
1826.597983	20.165556	63.232910
1825.965041	29.848957	63.237914
1825.202556	28.711689	63.242919
1824.678017	20.309678	63.247924
1823.862037	21.872685	63.252929
1823.563940	20.524493	63.257934
1822.745696	21.797710	63.262938
1822.309080	17.636234	63.267943
1821.984469	9.199331	63.272948
1821.188693	22.466081	63.277953
1821.168434	18.082383	63.282958
1819.557797	20.318754	63.287962
1818.263729	27.390118	63.292967
1817.831163	28.307217	63.297972
1817.239133	30.165818	63.302977
1817.501562	16.001412	63.307982
1816.881974	21.059200	63.312986
1816.029168	23.140552	63.317991
1815.593721	20.349224	63.322996
1814.141078	24.586837	63.328001
1813.129689	16.355171	63.333006
1812.566293	17.767692	63.338010
1812.000925	19.685137	63.343015
1811.961164	18.732730	63.348020
1810.900404	21.277598	63.353025
1810.525987	15.589266	63.358030
1809.855170	7.521143	63.363034
1809.454269	9.626930	63.368039
1808.957051	18.993894	63.373044
1807.563954	29.501298	63.378049
1807.106004	19.801962	63.383054
1806.325636	26.015925	63.388058
1805.679903	22.258230	63.393063
1805.572515	22.414088	63.398068
1804.661404	25.261617	63.403073
1804.176369	13.086113	63.408078
1803.160330	16.984751	63.413082
1802.097572	22.656945	63.418087
1801.811538	16.159819	63.423092
1800.938388	21.221604	63.428097
1800.689637	15.445512	63.433102
1800.096756	18.702967	63.438106
1799.545432	10.609564	63.443111
1798.643974	11.325160	63.448116
1797.458046	23.969490	63.453121
1796.775011	18.964081	63.458126
1796.373050	20.866620	63.463130
1795.652056	12.446932	63.468135
1795.566449	16.921630	63.473140
1794.761737	22.808309	63.478145
1794.705642	15.524066	63.483150
1793.430215	21.431875	63.488154
1792.233474	23.167314	63.493159
1791.433202	20.490690	63.498164
1790.889607	24.366353	63.503169
1790.668583	11.426709	63.508174
1790.166272	27.988330	63.513178
1789.706930	11.158456	63.518183
1789.606426	15.826324	63.523188
1788.129938	22.399979	63.528193
1787.557204	21.946931	63.533198
1786.557613	7.943512	63.538202
1786.267994	11.901841	63.543207
1785.470549	21.158792	63.548212
1784.166135	14.534809	63.553217
1783.520442	11.493032	63.558222
1782.935214	19.427952	63.563226
1782.607351	27.251047	63.568231
1782.296399	15.669205	63.573236
1781.481006	19.824564	63.578241
1780.961982	15.750299	63.583246
1780.746729	26.420749	63.588250
1779.783188	26.259989	63.593255
1778.804779	20.659689	63.598260
1777.937728	22.292319	63.603265
1777.569254	8.975561	63.608270
1776.979802	20.239998	63.613274
1775.997777	15.173269	63.618279
1775.036558	24.599729	63.623284
1774.201938	20.648118	63.628289
1773.968742	13.136542	63.633294
1773.327927	16.452074	63.638298
1772.852361	36.101769	63.643303
1772.366916	18.500199	63.648308
1771.925939	18.075116	63.653313
1771.618712	20.159727	63.658318
1770.561233	26.274205	63.663322
1769.480213	22.688142	63.668327
1769.175731	13.159987	63.673332
1768.325417	14.389428	63.678337
1767.174488	8.579998	63.683342
1766.100434	14.372262	63.688346
1766.046733	31.452410	63.693351
1765.527724	9.414038	63.698356
1764.502087	15.841992	63.703361
1764.196572	14.113376	63.708366
1763.742113	6.179640	63.713370
1763.455749	12.114891	63.718375
1763.145422	13.327966	63.723380
1761.721075	18.403178	63.728385
1761.275874	21.321807	63.733390
1760.426121	8.718552	63.738394
1759.792416	11.922573	63.743399
1758.622709	12.914164	63.748404
1757.835183	22.297275	63.753409
1757.532596	6.828624	63.758414
1756.987694	15.368980	63.763418
1756.464940	7.137018	63.768423
1756.253563	31.882306	63.773428
1755.785304	13.815985	63.778433
1754.801814	11.816579	63.783438
1754.000599	12.757538	63.788442
1753.264599	13.107840	63.793447
1752.456650	6.860762	63.798452
1751.197969	20.298802	63.803457
1750.902447	20.877188	63.808462
1750.185236	19.511988	63.813466
1750.140153	21.058246	63.818471
1749.743855	6.500161	63.823476
1748.141405	13.108028	63.828481
1747.506015	3.410092	63.833486
1746.834277	12.735388	63.838490
1746.244578	20.216875	63.843495
1746.152138	9.603257	63.848500
1745.756959	9.528863	63.853505
1744.334390	12.798244	63.858510
1743.393351	10.000495	63.863514
1742.762983	15.722306	63.868519
1742.434489	10.966532	63.873524
1742.012734	15.745340	63.878529
1741.543685	8.895683	63.883534
1741.290503	15.588888	63.888538
1739.782188	22.049354	63.893543
1739.284616	6.217448	63.898548
1738.515441	21.522075	63.903553
1738.263803	17.183012	63.908558
1736.800366	20.335890	63.913562
1735.956354	19.771400	63.918567
1735.576498	10.196879	63.923572
1734.935289	13.130870	63.928577
1734.680376	15.006908	63.933582
1734.099904	16.663423	63.938586
1733.376812	18.746276	63.943591
1733.360538	5.860862	63.948596
1732.057233	22.529187	63.953601
1731.351510	13.228762	63.958606
1730.890132	22.777694	63.963610
1730.295126	14.161407	63.968615
1729.105921	0.319023	63.973620
1728.342876	10.768961	63.978625
1727.777045	11.412356	63.983630
1727.270566	15.357824	63.988634
1726.911365	18.649140	63.993639
1726.765817	12.080835	63.998644
1725.136178	14.290317	64.003649
1724.444907	24.162758	64.008654
1724.268631	11.329560	64.013658
1723.559131	9.674571	64.018663
1722.750801	-0.085772	64.023668
1721.390107	17.299694	64.028673
1720.932078	18.096275	64.033678
1720.625411	10.798222	64.038682
1720.034389	12.990985	64.043687
1719.761779	4.433889	64.048692
1719.417793	14.531857	64.053697
1718.630353	-1.985679	64.058702
1717.841792	13.031871	64.063706
1716.932338	19.198546	64.068711
1715.662798	15.388569	64.073716
1714.809706	13.239163	64.078721
1714.365131	13.568421	64.083726
1714.013409	11.791959	64.088730
1713.433460	5.328919	64.093735
1713.026317	11.713849	64.098740
1712.351400	21.753998	64.103745
1712.022907	14.620256	64.108750
1711.128018	11.204928	64.113754
1710.282203	9.256212	64.118759
1709.791193	1.664179	64.123764
1708.943054	2.628372	64.128769
1707.971886	27.197858	64.133774
1707.394200	-12.484579	64.138778
1706.462324	24.651298	64.143783
1706.383786	-23.761281	64.148788
1705.480629	25.174712	64.153793
1705.128069	-1.395270	64.158798
1704.350729	12.890394	64.163802
1703.196098	19.699967	64.168807
1702.985523	2.330745	64.173812
1702.381694	11.612147	64.178817
1701.968380	3.783854	64.183822
1701.366360	4.117622	64.188826
1699.991994	17.053671	64.193831
1699.455793	4.667144	64.198836
1699.006848	7.340377	64.203841
1698.450226	12.851793	64.208846
1697.524115	10.892180	64.213850
1696.822618	1.045495	64.218855
1696.311026	14.770153	64.223860
1695.978935	12.523812	64.228865
1695.378724	8.911882	64.233870
1694.357480	21.263588	64.238874
1693.911524	10.113211	64.243879
1692.988398	-10.613582	64.248884
1692.410894	27.814268	64.253889
1692.003189	-5.865089	64.258894
1690.909098	20.589386	64.263898
1690.104227	8.981946	64.268903
1689.899229	6.182427	64.273908
1689.385510	15.089987	64.278913
1688.418671	0.371819	64.283918
1687.546634	12.266174	64.288922
1686.545430	19.813028	64.293927
1686.554550	3.257290	64.298932
1685.722033	8.102920	64.303937
1685.725764	2.196867	64.308942
1684.718525	10.209862	64.313946
1683.527490	17.126146	64.318951
1683.459581	12.281685	64.323956
1682.587522	16.177996	64.328961
1681.578639	-0.000010	64.333966
1680.637410	-0.008162	64.338970
1680.031381	17.101338	64.343975
1680.071898	2.056019	64.348980
1679.237825	19.878235	64.353985
1679.006193	18.938961	64.358990
1677.839214	11.845370	64.363994
1677.180794	11.434342	64.368999
1676.563585	6.986205	64.374004
1676.266886	12.691297	64.379009
1675.485395	9.276895	64.384014
1674.350754	15.356349	64.389018
1673.652674	14.177362	64.394023
1673.244343	8.246874	64.399028
1672.916389	11.619961	64.404033
1672.043963	19.278825	64.409038
1670.916014	12.776685	64.414042
1670.132923	18.664690	64.419047
1670.175460	14.223720	64.424052
1669.537166	25.615774	64.429057
1668.910022	6.451977	64.434062
1667.767713	17.398974	64.439066
1667.108711	12.970092	64.444071
1667.114266	10.514010	64.449076
1666.199644	14.447048	64.454081
1665.005255	5.561728	64.459086
1664.468967	5.935524	64.464090
1663.767214	17.851724	64.469095
1663.437320	3.074971	64.474100
1663.013050	20.097259	64.479105
1662.229565	11.741162	64.484110
1661.314280	14.240901	64.489114
1660.436814	15.357998	64.494119
1660.238894	14.325065	64.499124
1659.636364	13.838934	64.504129
1658.834829	11.738126	64.509134
1658.065172	14.766651	64.514138
1657.447449	10.604019	64.519143
1656.956269	7.280700	64.524148
1655.683621	17.701220	64.529153
1654.732873	14.365747	64.534158
1654.318629	7.538944	64.539162
1654.054203	15.974838	64.544167
1653.550316	9.559654	64.549172
1653.036996	14.334093	64.554177
1652.485914	11.105442	64.559182
1651.936689	7.550078	64.564186
1650.943299	19.170418	64.569191
1650.538267	4.615331	64.574196
1649.528443	6.986592	64.579201
1648.564960	0.649149	64.584206
1648.187810	0.384255	64.589210
1647.248313	14.862838	64.594215
1646.650966	2.881847	64.599220
1645.271260	13.536986	64.604225
1645.344954	7.842163	64.609230
1644.848707	19.091807	64.614234
1643.864955	10.594070	64.619239
1643.791197	11.537775	64.624244
1643.086156	15.546334	64.629249
1642.773910	18.205747	64.634254
1641.519226	15.267054	64.639258
1640.651350	5.766928	64.644263
1640.756079	7.082812	64.649268
1639.401464	18.937148	64.654273
1638.421807	13.609914	64.659278
1637.703516	9.165229	64.664282
1637.127776	16.061058	64.669287
1637.061136	7.466527	64.674292
1636.784137	10.155032	64.679297
1636.048132	7.718981	64.684302
1635.138296	12.781906	64.689306
1634.269913	14.047374	64.694311
1633.993222	7.583490	64.699316
1632.573187	18.044778	64.704321
1632.076992	4.442435	64.709326
1631.485053	11.694062	64.714330
1630.788688	16.314662	64.719335
1630.724959	8.282622	64.724340
1630.222248	7.045805	64.729345
1629.229831	12.454576	64.734350
1628.720841	16.392573	64.739354
1627.788505	15.870534	64.744359
1626.704148	3.482804	64.749364
1625.503605	10.023737	64.754369
1625.578649	5.993909	64.759374
1625.292247	8.682332	64.764378
1624.361428	20.800502	64.769383
1624.458025	10.197873	64.774388
1622.962743	11.230204	64.779393
1622.336789	11.700251	64.784398
1622.082819	8.109030	64.789402
1620.981994	9.562809	64.794407
1620.332477	6.002886	64.799412
1619.615872	8.460038	64.804417
1619.203276	5.507432	64.809422
1618.918547	6.921452	64.814426
1617.693541	6.535793	64.819431
1617.191634	5.395042	64.824436
1616.137804	7.738614	64.829441
1615.913266	11.114201	64.834446
1615.545864	2.422379	64.839450
1614.209821	7.619244	64.844455
1613.727303	-4.250664	64.849460
1612.829144	5.694070	64.854465
1612.815192	4.847952	64.859470
1612.138505	12.705961	64.864474
1610.968057	10.474547	64.869479
1610.560467	6.185511	64.874484
1609.829696	3.478987	64.879489
1609.406272	6.419405	64.884494
1608.688811	7.153143	64.889498
1607.567108	11.835008	64.894503
1607.152975	7.539127	64.899508
1606.504746	6.473662	64.904513
1606.066073	9.556847	64.909518
1605.356159	21.236242	64.914522
1604.252381	18.049674	64.919527
1603.843190	1.312833	64.924532
1603.203638	21.895272	64.929537
1602.828998	11.802731	64.934542
1601.845306	16.084218	64.939546
1601.102424	12.548592	64.944551
1600.604441	5.552187	64.949556
1600.173757	8.358146	64.954561
1599.838677	10.988074	64.959566
1598.698858	7.832467	64.964570
1597.722001	11.114690	64.969575
1597.630617	7.754678	64.974580
1596.828873	13.339742	64.979585
1595.811306	3.193235	64.984590
1595.496588	2.308170	64.989594
1594.982477	18.535777	64.994599
1594.589464	2.165363	64.999604
1593.268301	1.265153	65.004609
1592.723841	12.576070	65.009614
1592.122690	2.369718	65.014618
1590.771243	9.514938	65.019623
1590.313938	12.342475	65.024628
1589.354962	21.528936	65.029633
1589.343753	4.112301	65.034638
1588.747690	-0.742854	65.039642
1588.294998	19.942356	65.044647
1588.102260	-1.204768	65.049652
1587.276790	6.885029	65.054657
1586.602306	7.244527	65.059662
1585.474968	10.799812	65.064666
1584.231326	13.019016	65.069671
1583.556460	0.941559	65.074676
1583.246879	10.941025	65.079681
1582.733698	2.234525	65.084686
1582.388424	11.060140	65.089690
1581.702094	5.191186	65.094695
1581.186968	1.302429	65.099700
1580.254463	2.138145	65.104705
1579.628367	5.598028	65.109710
1578.610951	-0.240399	65.114714
1577.564570	16.090692	65.119719
1577.229358	10.309452	65.124724
1576.952267	12.075489	65.129729
1576.642990	12.943075	65.134734
1576.009124	9.576213	65.139738
1575.150187	9.502987	65.144743
1574.700184	5.069315	65.149748
1573.292840	8.385247	65.154753
1572.266629	8.493134	65.159758
1572.135287	6.724257	65.164762
1571.162199	3.335601	65.169767
1570.885662	-0.064375	65.174772
1570.316947	14.602888	65.179777
1569.833603	7.943198	65.184782
1568.994281	9.867944	65.189786
1568.312419	5.400149	65.194791
1567.845719	6.434669	65.199796
1567.189458	8.502213	65.204801
1566.203997	2.806943	65.209806
1565.555822	6.292413	65.214810
1564.785422	11.222822	65.219815
1565.008330	-3.964988	65.224820
1563.536698	9.376054	65.229825
1562.661139	15.982072	65.234830
1562.537359	0.906108	65.239834
1561.685807	13.358610	65.244839
1561.389438	-0.934596	65.249844
1560.225186	3.610547	65.254849
1559.710182	8.348996	65.259854
1559.093502	12.580070	65.264858
1557.944588	16.881515	65.269863
1557.331405	5.893364	65.274868
1556.580199	7.881382	65.279873
1555.972666	3.859083	65.284878
1555.838816	0.327633	65.289882
1555.094693	13.321291	65.294887
1555.072844	5.206917	65.299892
1554.157046	11.409334	65.304897
1553.282284	9.446349	65.309902
1552.686972	6.172713	65.314906
1551.474581	7.417173	65.319911
1551.004172	2.362296	65.324916
1550.307220	14.684586	65.329921
1549.947509	10.744333	65.334926
1549.525382	3.925118	65.339930
1548.341540	12.852432	65.344935
1548.226995	1.807139	65.349940
1547.668463	17.942459	65.354945
1546.504073	7.352539	65.359950
1545.729569	1.901294	65.364954
1545.041391	17.727641	65.369959
1544.547425	7.434888	65.374964
1543.587786	10.649741	65.379969
1542.715187	16.682879	65.384974
1542.289052	2.935401	65.389978
1541.739965	13.485415	65.394983
1541.598433	2.373450	65.399988
1540.763273	6.317552	65.404993
1539.914273	-0.413335	65.409998
1539.421812	-3.651269	65.415002
1538.564167	3.349282	65.420007
1538.064123	7.265369	65.425012
1537.020749	13.910672	65.430017
1536.336234	21.768365	65.435022
1536.041338	19.601290	65.440026
1535.408523	2.508931	65.445031
1534.909290	5.212254	65.450036
1533.632084	14.283715	65.455041
1533.328534	9.722705	65.460046
1532.960726	1.981839	65.465050
1531.615104	9.233388	65.470055
1531.079924	20.497111	65.475060
1530.131796	11.377199	65.480065
1529.855868	10.280982	65.485070
1529.926259	7.019845	65.490074
1528.658783	8.244684	65.495079
1528.033947	2.077405	65.500084
1527.293432	12.930640	65.505089
1526.639221	11.560227	65.510094
1526.377291	6.642534	65.515098
1525.130125	21.206303	65.520103
1524.897218	13.898144	65.525108
1524.466878	9.708931	65.530113
1523.311833	7.596533	65.535118
1522.427016	3.167309	65.540122
1521.813054	3.526669	65.545127
1521.504161	3.998398	65.550132
1521.178615	10.463416	65.555137
1519.970671	13.454389	65.560142
1519.246892	9.564107	65.565146
1518.642561	9.625479	65.570151
1518.429935	11.322933	65.575156
1517.478042	16.726879	65.580161
1516.290175	12.306386	65.585166
1515.978526	13.868192	65.590170
1515.413723	13.013413	65.595175
1515.285932	4.084852	65.600180
1514.057902	15.867082	65.605185
1513.132384	8.657945	65.610190
1512.666591	8.596384	65.615194
1512.125036	6.047475	65.620199
1511.714689	5.754762	65.625204
1510.740840	15.329944	65.630209
1509.982215	14.666808	65.635214
1510.098834	15.192347	65.640218
1509.057786	3.116335	65.645223
1508.385946	10.591980	65.650228
1507.563801	19.318342	65.655233
1507.068189	7.999299	65.660238
1505.809484	6.797483	65.665242
1504.808213	-2.826456	65.670247
1504.329185	-8.852894	65.675252
1503.794348	16.940317	65.680257
1503.325708	10.691454	65.685262
1503.248427	0.330930	65.690266
1502.926568	18.027619	65.695271
1502.630766	1.829441	65.700276
1501.667288	15.021961	65.705281
1500.221047	-2.275424	65.710286
1499.675028	5.735295	65.715290
1498.954200	3.739985	65.720295
1498.711458	3.335488	65.725300
1497.374012	17.934108	65.730305
1496.674230	3.302910	65.735310
1496.134592	2.286448	65.740314
1495.881167	23.039337	65.745319
1495.300323	-0.540744	65.750324
1493.758231	5.882631	65.755329
1493.320432	13.761044	65.760334
1493.136667	2.190613	65.765338
1492.368591	20.335090	65.770343
1491.217377	16.545852	65.775348
1490.879634	10.575803	65.780353
1490.203995	1.604997	65.785358
1490.193152	15.300553	65.790362
1489.362365	6.881083	65.795367
1488.631279	6.858530	65.800372
1487.833039	2.497561	65.805377
1487.164797	5.916853	65.810382
1486.069135	15.429400	65.815386
1485.227154	15.321972	65.820391
1484.921770	6.256060	65.825396
1484.198303	4.652244	65.830401
1484.241806	24.104314	65.835406
1484.046319	4.875163	65.840410
1482.518336	14.306605	65.845415
1481.948964	-1.133755	65.850420
1481.111858	14.985910	65.855425
1480.098155	12.682343	65.860430
1479.644399	-1.106452	65.865434
1479.066226	9.214806	65.870439
1478.696229	6.872024	65.875444
1477.536454	14.363716	65.880449
1476.785663	11.411264	65.885454
1476.521874	-1.712305	65.890458
1475.727467	7.455911	65.895463
1475.425006	7.642782	65.900468
1474.207069	14.587073	65.905473
1473.323406	-8.487562	65.910478
1472.874443	8.959664	65.915482
1472.679116	7.505304	65.920487
1472.472883	8.306066	65.925492
1471.806158	-5.969255	65.930497
1470.858723	6.809145	65.935502
1470.036877	18.517382	65.940506
1468.900490	-7.456431	65.945511
1468.162976	22.274970	65.950516
1467.674729	-0.607053	65.955521
1467.152228	19.728133	65.960526
1467.183682	12.762738	65.965530
1466.057276	2.097448	65.970535
1464.925985	23.041878	65.975540
1464.524134	11.949211	65.980545
1464.176812	3.222696	65.985550
1463.291959	1.280271	65.990554
1462.057290	21.950979	65.995559
1461.984536	4.769646	66.000564
1461.276053	2.354507	66.005569
1461.211331	7.740478	66.010574
1460.239916	9.817133	66.015578
1459.319238	9.466761	66.020583
1458.888149	1.139901	66.025588
1457.796650	2.819338	66.030593
1457.043354	18.711234	66.035598
1456.598843	1.577947	66.040602
1456.055757	15.946265	66.045607
1455.978238	4.128727	66.050612
1454.777084	-2.932499	66.055617
1454.113861	12.352163	66.060622
1453.751093	-8.286933	66.065626
1452.600972	10.943234	66.070631
1451.775708	4.423067	66.075636
1451.204412	8.221185	66.080641
1450.499223	-7.785755	66.085646
1450.256114	17.924823	66.090650
1449.412212	-1.272223	66.095655
1448.389456	-1.292565	66.100660
1448.044659	7.305903	66.105665
1447.427488	6.823726	66.110670
1447.326805	7.161453	66.115674
1446.075969	-5.761086	66.120679
1445.608923	13.163416	66.125684
1444.906389	8.063454	66.130689
1444.158777	-8.119660	66.135694
1443.324868	14.040594	66.140698
1442.769809	-11.673931	66.145703
1442.222537	9.739044	66.150708
1441.765402	6.844011	66.155713
1440.052264	13.455444	66.160718
1440.010673	3.655361	66.165722
1439.205376	0.487667	66.170727
1438.916182	0.539974	66.175732
1438.766205	10.452576	66.180737
1437.382538	-16.305040	66.185742
1436.959314	15.032136	66.190746
1436.433046	-5.268747	66.195751
1435.866612	14.202967	66.200756
1434.834121	-6.268188	66.205761
1434.187804	14.553430	66.210766
1433.995566	0.437667	66.215770
1432.773751	10.706689	66.220775
1431.678789	1.200172	66.225780
1431.412623	7.936444	66.230785
1431.039511	5.545282	66.235790
1431.087944	-9.173251	66.240794
1429.206070	-0.970719	66.245799
1428.768392	-0.412281	66.250804
1428.342683	3.720657	66.255809
1427.886635	11.650860	66.260814
1427.115319	3.616191	66.265818
1426.046061	-1.977392	66.270823
1425.596784	7.487630	66.275828
1425.196049	-0.158094	66.280833
1424.209130	0.985936	66.285838
1423.530248	4.244512	66.290842
1422.920512	0.724055	66.295847
1422.670777	-5.625801	66.300852
1421.814567	-2.815265	66.305857
1420.720196	4.897852	66.310862
1419.848478	0.217437	66.315866
1419.352384	4.992323	66.320871
1419.124625	-6.739822	66.325876
1418.951617	5.854006	66.330881
1417.564164	0.638994	66.335886
1417.069079	0.176843	66.340890
1416.566570	6.006117	66.345895
1416.214665	3.168479	66.350900
1415.182792	4.929916	66.355905
1414.530606	0.052192	66.360910
1414.155022	-13.406808	66.365914
1412.796025	-0.895714	66.370919
1412.609668	4.651507	66.375924
1411.866863	6.874763	66.380929
1410.974633	6.694924	66.385934
1410.303924	-6.051724	66.390938
1409.366715	3.643806	66.395943
1409.293384	4.746713	66.400948
1408.685379	0.560534	66.405953
1407.975956	5.563286	66.410958
1407.152812	3.056005	66.415962
1406.281545	0.302493	66.420967
1406.117776	3.260013	66.425972
1405.293654	14.653242	66.430977
1404.373433	4.242209	66.435982
1403.951792	2.323950	66.440986
1403.187884	-1.231919	66.445991
1402.638711	-7.091071	66.450996
1401.576873	11.082748	66.456001
1400.851155	1.148566	66.461006
1400.228702	2.166869	66.466010
1400.168739	4.103407	66.471015
1399.598326	6.882718	66.476020
1398.377626	1.658559	66.481025
1397.725080	-4.412812	66.486030
1397.871578	-1.559799	66.491034
1396.892750	4.360952	66.496039
1395.729098	-3.562458	66.501044
1395.275173	-3.646383	66.506049
1394.699725	-3.127542	66.511054
1393.694657	-2.057884	66.516058
1393.129332	9.174365	66.521063
1392.534810	-7.274325	66.526068
1392.355085	1.905010	66.531073
1391.142464	8.096306	66.536078
1390.560018	-1.836989	66.541082
1389.723224	0.995701	66.546087
1389.308506	-1.425108	66.551092
1389.201324	14.403516	66.556097
1388.241082	7.135301	66.561102
1387.419985	-0.774747	66.566106
1386.761822	7.323195	66.571111
1386.073329	1.863067	66.576116
1384.781154	4.679835	66.581121
1384.302985	2.944023	66.586126
1384.124482	5.946462	66.591130
1383.683980	7.281190	66.596135
1382.667923	5.903677	66.601140
1381.799998	1.419787	66.606145
1381.162401	0.715377	66.611150
1380.966330	12.363582	66.616154
1380.270780	10.820013	66.621159
1379.348616	-4.452268	66.626164
1378.901113	9.992315	66.631169
1378.271204	0.758825	66.636174
1377.826010	-4.408822	66.641178
1376.453349	13.224651	66.646183
1375.648836	11.289986	66.651188
1375.181965	14.801872	66.656193
1374.621621	8.681155	66.661198
1374.471376	2.362796	66.666202
1373.671887	14.531103	66.671207
1372.997384	-0.868851	66.676212
1372.283204	10.997321	66.681217
1371.422921	8.672567	66.686222
1370.927985	0.795833	66.691226
1370.313546	10.332844	66.696231
1369.708270	3.511246	66.701236
1368.600469	1.818751	66.706241
1367.837267	22.286813	66.711246
1367.488263	8.424627	66.716250
1367.362987	3.340164	66.721255
1366.627242	-1.666184	66.726260
1365.739624	-3.434675	66.731265
1364.844274	5.900990	66.736270
1363.965878	0.095755	66.741274
1363.032104	16.837911	66.746279
1362.343777	2.627560	66.751284
1361.868125	4.634905	66.756289
1361.414988	-0.813741	66.761294
1361.484462	20.744054	66.766298
1360.606958	2.462263	66.771303
1360.133244	-2.797038	66.776308
1359.082815	15.315060	66.781313
1358.051972	-7.393924	66.786318
1357.398207	30.202346	66.791322
1356.420189	4.334303	66.796327
1356.467710	8.942364	66.801332
1356.112048	-5.945307	66.806337
1355.102901	17.846519	66.811342
1354.455438	1.906127	66.816346
1353.494168	7.098730	66.821351
1353.631705	-3.194996	66.826356
1352.368352	19.013037	66.831361
1351.285149	24.888904	66.836366
1351.151346	9.193272	66.841370
1350.419606	6.928514	66.846375
1349.261466	6.123938	66.851380
1348.601845	6.167332	66.856385
1348.119642	23.131018	66.861390
1348.129515	12.259931	66.866394
1347.307926	-0.740246	66.871399
1346.638308	6.407078	66.876404
1346.008432	-0.790632	66.881409
1345.048519	6.153689	66.886414
1344.568937	14.205909	66.891418
1343.590623	8.140605	66.896423
1342.726065	0.166523	66.901428
1342.778467	11.626999	66.906433
1341.528024	8.845478	66.911438
1341.028526	-7.447990	66.916442
1340.320004	14.686034	66.921447
1340.039556	14.194509	66.926452
1339.396837	-7.585870	66.931457
1338.481491	19.909369	66.936462
1338.060108	-9.364916	66.941466
1337.219450	4.140832	66.946471
1336.396667	20.318169	66.951476
1335.532813	2.669711	66.956481
1334.559984	13.801175	66.961486
1334.761235	1.144588	66.966490
1334.174450	0.009505	66.971495
1332.990789	15.151416	66.976500
1332.337594	0.618539	66.981505
1331.446084	2.602114	66.986510
1331.396042	19.298406	66.991514
1330.824537	11.146854	66.996519
1330.001868	14.194931	67.001524
1329.130347	6.367033	67.006529
1328.594006	5.063088	67.011534
1328.213961	6.780860	67.016538
1327.129533	-0.074935	67.021543
1326.538687	8.710881	67.026548
1326.110159	16.967869	67.031553
1325.440141	-4.249946	67.036558
1324.981942	0.011167	67.041562
1323.888466	8.143630	67.046567
1323.728214	9.637235	67.051572
1322.635675	14.505378	67.056577
1321.614388	14.916923	67.061582
1321.432714	-2.560858	67.066586
1320.612947	9.806213	67.071591
1319.673985	5.723131	67.076596
1319.174052	8.800325	67.081601
1318.667798	12.163944	67.086606
1318.185048	10.280644	67.091610
1317.448880	0.116353	67.096615
1316.524674	-4.602982	67.101620
1316.062882	16.301266	67.106625
1315.429773	-2.517647	67.111630
1315.075212	0.921199	67.116634
1313.558542	17.710300	67.121639
1313.233477	7.447535	67.126644
1312.850277	8.432554	67.131649
1311.972337	4.918496	67.136654
1311.092995	14.690012	67.141658
1309.935796	4.904880	67.146663
1309.931165	4.855194	67.151668
1309.529369	4.908071	67.156673
1309.000703	4.484395	67.161678
1308.856703	14.839151	67.166682
1307.550985	12.004936	67.171687
1306.812600	-2.768265	67.176692
1305.998084	11.688938	67.181697
1305.166525	2.405531	67.186702
1304.588313	-0.374033	67.191706
1304.131568	10.462509	67.196711
1304.009818	9.420652	67.201716
1302.999707	-5.034966	67.206721
1302.279417	24.687387	67.211726
1302.093865	-19.713679	67.216730
1300.512075	16.650303	67.221735
1299.805467	1.496748	67.226740
1299.225286	4.211402	67.231745
1298.894787	3.473959	67.236750
1298.759979	-0.082546	67.241754
1297.646019	4.702280	67.246759
1297.121134	4.814150	67.251764
1296.160854	-2.040866	67.256769
1294.740168	-0.879865	67.261774
1294.404936	0.611598	67.266778
1293.909537	5.012667	67.271783
1293.632632	7.970832	67.276788
1293.122901	5.590375	67.281793
1292.717491	7.474605	67.286798
1291.878285	1.227945	67.291802
1290.915357	17.645178	67.296807
1290.198541	5.642309	67.301812
1289.349795	10.154748	67.306817
1288.562416	-8.915574	67.311822
1288.574735	8.101932	67.316826
1287.799017	19.072768	67.321831
1287.228050	4.187800	67.326836
1286.374248	6.476043	67.331841
1285.290809	8.535878	67.336846
1285.254929	6.892188	67.341850
1284.086911	9.493730	67.346855
1283.272736	5.048638	67.351860
1282.816435	-6.363301	67.356865
1282.051307	-3.335400	67.361870
1281.937508	-1.527494	67.366874
1281.458216	4.555139	67.371879
1280.867981	10.850948	67.376884
1279.915578	12.675495	67.381889
1278.936948	-3.365166	67.386894
1278.073120	-6.250694	67.391898
1277.492059	8.467426	67.396903
1277.302414	-14.804151	67.401908
1276.301921	18.416133	67.406913
1275.502738	1.856523	67.411918
1274.959708	-4.481370	67.416922
1274.386516	8.245459	67.421927
1274.259407	6.688812	67.426932
1273.332192	1.392827	67.431937
1272.234485	3.544818	67.436942
1272.064871	5.684863	67.441946
1270.881564	21.090084	67.446951
1270.103883	-8.794547	67.451956
1269.625010	18.394762	67.456961
1269.017194	0.609443	67.461966
1268.771239	8.782212	67.466970
1267.882382	-8.117927	67.471975
1266.959899	26.559638	67.476980
1266.691087	1.231737	67.481985
1266.086669	22.297433	67.486990
1264.846331	1.542465	67.491994
1264.318979	3.103900	67.496999
1263.817662	16.634564	67.502004
1263.443238	-15.291594	67.507009
1262.745203	10.128580	67.512014
1261.856817	6.201478	67.517018
1261.268727	12.470142	67.522023
1260.647011	-4.638044	67.527028
1259.833458	13.103684	67.532033
1259.382615	12.741759	67.537038
1258.687763	-0.697982	67.542042
1257.952252	20.837971	67.547047
1256.609393	6.875227	67.552052
1256.467767	-6.106863	67.557057
1255.845776	1.390857	67.562062
1255.750412	13.701110	67.567066
1254.555095	-13.185650	67.572071
1253.980784	9.415866	67.577076
1253.692237	-15.700713	67.582081
1252.338730	24.316931	67.587086
1251.873149	-5.704049	67.592090
1250.890928	21.163187	67.597095
1250.774756	3.069476	67.602100
1250.187481	15.606171	67.607105
1249.693788	-7.112458	67.612110
1248.552231	19.647651	67.617114
1247.494217	-3.359712	67.622119
1247.456731	6.117115	67.627124
1246.824273	4.140945	67.632129
1245.497348	10.795159	67.637134
1245.031903	7.236038	67.642138
1244.503250	9.026334	67.647143
1243.995758	19.632843	67.652148
1243.764077	-4.283313	67.657153
1242.657538	27.708108	67.662158
1242.325785	-6.845645	67.667162
1241.510276	33.222094	67.672167
1240.139933	-2.024362	67.677172
1239.886026	-5.260736	67.682177
1239.163910	15.946663	67.687182
1239.229852	-17.328359	67.692186
1238.494057	25.848930	67.697191
1238.102348	-8.266368	67.702196
1236.922232	7.078419	67.707201
1236.199015	10.779312	67.712206
1235.412284	-6.949150	67.717210
1234.353330	13.736240	67.722215
1234.646317	-23.556529	67.727220
1233.633930	18.855773	67.732225
1232.607035	-4.058758	67.737230
1232.042859	17.565061	67.742234
1231.905508	-18.575966	67.747239
1230.765482	7.942616	67.752244
1229.959599	-11.682949	67.757249
1229.066929	15.974255	67.762254
1229.163502	2.545871	67.767258
1228.098392	4.762079	67.772263
1227.687588	7.058745	67.777268
1226.885486	5.883810	67.782273
1226.386852	-16.029793	67.787278
1225.564382	10.570760	67.792282
1224.553013	-9.148284	67.797287
1224.290837	13.812020	67.802292
1223.894004	-14.330738	67.807297
1222.618651	21.647091	67.812302
1222.065311	-6.525986	67.817306
1220.881578	15.123808	67.822311
1221.009728	3.382412	67.827316
1220.752991	10.060423	67.832321
1219.746322	-0.625344	67.837326
1218.665680	12.232644	67.842330
1218.342184	-8.731141	67.847335
1218.046501	19.192250	67.852340
1216.869558	-16.453895	67.857345
1216.059292	10.936317	67.862350
1215.412250	-9.591255	67.867354
1215.178953	11.125264	67.872359
1214.848395	-12.128620	67.877364
1213.709991	14.000226	67.882369
1213.052517	0.008955	67.887374
1212.157936	-6.427554	67.892378
1210.993785	22.214238	67.897383
1210.634237	0.795721	67.902388
1210.111928	14.225648	67.907393
1209.816872	3.453533	67.912398
1209.337581	9.293335	67.917402
1208.114978	16.938615	67.922407
1207.848536	-17.368446	67.927412
1207.400357	24.312357	67.932417
1206.685871	-10.987877	67.937422
1205.345982	8.464901	67.942426
1204.904413	2.990798	67.947431
1204.470451	-2.241671	67.952436
1203.942694	13.904532	67.957441
1203.090527	-5.934432	67.962446
1202.680032	-20.710824	67.967450
1201.951581	14.101428	67.972455
1201.178734	-28.695496	67.977460
1200.243738	17.553682	67.982465
1199.294785	18.710682	67.987470
1199.483951	-16.165550	67.992474
1198.495806	18.997080	67.997479
1197.506879	-15.844771	68.002484
1197.000562	15.529228	68.007489
1196.490418	-15.399215	68.012494
1196.533110	6.963836	68.017498
1195.104279	-9.552362	68.022503
1194.659395	9.239299	68.027508
1194.220735	-3.064789	68.032513
1192.685847	0.610650	68.037518
1192.171929	13.810593	68.042522
1191.479731	-7.461968	68.047527
1191.026435	17.901953	68.052532
1190.949329	17.469569	68.057537
1189.901745	-13.229912	68.062542
1189.268596	10.388593	68.067546
1188.339547	3.170702	68.072551
1188.286115	-20.127228	68.077556
1187.253772	4.735841	68.082561
1186.394857	16.328605	68.087566
1186.206699	-14.562732	68.092570
1185.345768	-1.761763	68.097575
1184.444958	6.467836	68.102580
1183.667881	-6.859447	68.107585
1183.154691	3.431006	68.112590
1182.987515	5.138599	68.117594
1181.809476	6.284728	68.122599
1181.197057	2.883031	68.127604
1180.338844	-5.721167	68.132609
1179.616988	13.081429	68.137614
1180.084744	1.778021	68.142618
1178.605556	4.870622	68.147623
1178.227287	3.284540	68.152628
1177.529833	-1.868175	68.157633
1176.316481	18.187375	68.162638
1175.852793	-11.199943	68.167642
1175.089035	22.842111	68.172647
1174.638461	-4.123618	68.177652
1174.517551	4.257912	68.182657
1173.052755	20.920557	68.187662
1172.786802	-0.397714	68.192666
1172.047536	2.750678	68.197671
1171.669999	11.225061	68.202676
1170.573670	8.184163	68.207681
1169.656676	3.939961	68.212686
1169.575251	8.831857	68.217690
1168.938892	16.407575	68.222695
1167.740561	3.295511	68.227700
1167.425499	20.500685	68.232705
1166.632735	-2.955646	68.237710
1166.479855	23.546329	68.242714
1165.123567	8.392073	68.247719
1164.687386	3.618839	68.252724
1164.146237	3.145142	68.257729
1163.395359	12.196120	68.262734
1162.662459	10.108217	68.267738
1162.004692	3.126305	68.272743
1161.303501	4.379528	68.277748
1161.221058	23.818436	68.282753
1160.429545	15.235164	68.287758
1159.447144	9.306205	68.292762
1158.585045	16.701791	68.297767
1158.179414	3.427397	68.302772
1158.000959	6.177534	68.307777
1156.898103	14.429816	68.312782
1156.423054	9.167619	68.317786
1155.712733	11.299048	68.322791
1154.283884	-7.014777	68.327796
1154.023263	10.066612	68.332801
1153.483872	2.042473	68.337806
1153.318436	-7.496606	68.342810
1152.363343	3.455464	68.347815
1151.661168	10.604849	68.352820
1151.286111	18.501700	68.357825
1150.127734	11.312409	68.362830
1149.333421	6.449484	68.367834
1148.694573	3.083537	68.372839
1148.598976	10.279951	68.377844
1147.896171	6.656104	68.382849
1146.720851	12.184003	68.387854
1146.415912	4.220345	68.392858
1145.810203	12.552829	68.397863
1144.752873	7.674968	68.402868
1144.351061	6.625625	68.407873
1143.500755	13.623537	68.412878
1143.321774	2.965437	68.417882
1142.282762	1.304680	68.422887
1141.109328	1.573343	68.427892
1140.851339	2.327168	68.432897
1140.143269	-0.067438	68.437902
1139.984772	-0.291341	68.442906
1138.952954	3.277312	68.447911
1138.092818	-2.628501	68.452916
1137.693039	-0.538574	68.457921
1137.220677	-2.962782	68.462926
1136.648340	6.851402	68.467930
1135.756577	1.854177	68.472935
1134.874431	20.045214	68.477940
1134.789826	6.270352	68.482945
1133.442407	1.053874	68.487950
1133.133579	5.835284	68.492954
1132.168731	-1.018931	68.497959
1131.795519	9.730220	68.502964
1131.472326	3.483551	68.507969
1130.640049	9.277006	68.512974
1129.733312	1.036920	68.517978
1129.064095	7.931918	68.522983
1128.305942	-0.170955	68.527988
1127.684082	3.669954	68.532993
1127.127710	7.918326	68.537998
1126.855982	4.776259	68.543002
1125.359876	17.044369	68.548007
1124.558336	10.974700	68.553012
1124.401436	9.596259	68.558017
1123.623381	8.792834	68.563022
1123.499761	4.020358	68.568026
1122.782129	-2.313376	68.573031
1122.163766	-4.971393	68.578036
1121.665148	-2.802668	68.583041
1120.206616	7.073623	68.588046
1119.660507	2.007237	68.593050
1118.850050	3.310964	68.598055
1118.726836	5.355330	68.603060
1118.451300	-6.224076	68.608065
1116.975133	5.673441	68.613070
1116.430890	-9.007547	68.618074
1115.839727	-0.858722	68.623079
1115.288421	-3.593633	68.628084
1114.584654	0.067925	68.633089
1113.622236	2.105425	68.638094
1113.594567	8.510471	68.643098
1112.876591	-4.647994	68.648103
1111.947306	2.274178	68.653108
1111.469741	-0.174429	68.658113
1110.721534	4.025612	68.663118
1109.820525	-10.835161	68.668122
1109.308227	-1.483096	68.673127
1108.881073	-6.049600	68.678132
1108.428308	0.965506	68.683137
1106.907821	-0.257546	68.688142
1106.667325	-9.824098	68.693146
1105.728441	-1.287241	68.698151
1105.279282	10.798581	68.703156
1104.791890	-9.517798	68.708161
1103.702859	-1.767580	68.713166
1103.259717	-1.263411	68.718170
1102.456514	2.188471	68.723175
1102.276786	6.358015	68.728180
1101.100544	-5.303619	68.733185
1100.467328	-2.630953	68.738190
1100.272376	-2.612520	68.743194
1099.388882	2.495254	68.748199
1098.826371	1.370559	68.753204
1098.259925	-3.068136	68.758209
1097.314972	0.521406	68.763214
1096.977572	-3.253580	68.768218
1095.911910	3.827478	68.773223
1095.210700	4.385312	68.778228
1094.858160	-2.425937	68.783233
1094.012036	-3.775167	68.788238
1093.336904	5.539728	68.793242
1092.766266	-2.411614	68.798247
1091.986704	1.195776	68.803252
1091.926823	-5.452295	68.808257
1090.830435	-5.579048	68.813262
1089.926276	-15.465790	68.818266
1089.389979	-9.851871	68.823271
1089.195767	-6.600930	68.828276
1088.609057	-2.546417	68.833281
1087.357872	12.912221	68.838286
1086.859165	-7.481197	68.843290
1086.008644	4.711038	68.848295
1084.771533	5.686842	68.853300
1084.563517	-0.448831	68.858305
1084.145239	4.542373	68.863310
1083.869525	-2.328400	68.868314
1083.072744	-2.247351	68.873319
1082.023609	-0.248084	68.878324
1081.399868	-4.993038	68.883329
1081.020994	-0.306136	68.888334
1080.856827	0.123700	68.893338
1079.698779	-3.563322	68.898343
1078.591592	16.532131	68.903348
1078.483924	-4.923238	68.908353
1077.250492	4.808460	68.913358
1076.203582	-1.444497	68.918362
1076.220213	5.893326	68.923367
1075.846868	-7.053445	68.928372
1075.559266	4.114154	68.933377
1074.468148	-3.798543	68.938382
1073.721248	-5.601925	68.943386
1073.396173	-0.125673	68.948391
1072.033276	2.327192	68.953396
1071.457194	-5.281090	68.958401
1070.666074	16.024023	68.963406
1070.479922	-4.031195	68.968410
1070.013969	2.125031	68.973415
1068.989976	-2.270835	68.978420
1068.343140	-0.386017	68.983425
1067.673336	4.757159	68.988430
1067.183936	1.919375	68.993434
1066.389139	-1.476931	68.998439
1065.810291	4.421299	69.003444
1065.288855	-3.061639	69.008449
1063.797693	3.350707	69.013454
1063.490195	2.641176	69.018458
1062.901357	18.745067	69.023463
1062.815815	-3.431306	69.028468
1061.916880	1.932814	69.033473
1060.798110	15.053948	69.038478
1060.455602	-11.768059	69.043482
1060.022864	25.138580	69.048487
1059.308190	-0.632379	69.053492
1058.388095	4.667303	69.058497
1058.135996	-1.412469	69.063502
1057.278639	6.562679	69.068506
1056.012330	8.259050	69.073511
1055.415262	4.101192	69.078516
1055.290311	-6.598595	69.083521
1054.707070	-2.014793	69.088526
1053.922961	-5.414371	69.093530
1052.998574	3.968565	69.098535
1052.411895	-17.765380	69.103540
1052.077208	19.048377	69.108545
1051.117559	-10.892315	69.113550
1050.252876	18.763099	69.118554
1049.561251	-11.546644	69.123559
1048.986116	24.084862	69.128564
1048.758014	-2.247597	69.133569
1047.677967	-4.343314	69.138574
1047.148227	-0.375124	69.143578
1046.647316	2.590310	69.148583
1046.043150	-9.304214	69.153588
1045.093617	1.771571	69.158593
1044.307398	-10.097144	69.163598
1044.329370	-9.622803	69.168602
1043.604590	-10.677518	69.173607
1042.318935	-6.686844	69.178612
1042.033676	-10.716109	69.183617
1041.238371	-8.172180	69.188622
1040.736316	-0.967885	69.193626
1039.831166	1.666057	69.198631
1039.017370	-15.372042	69.203636
1038.585026	8.667081	69.208641
1038.359065	-6.037706	69.213646
1037.309167	-14.731188	69.218650
1036.672649	-8.462676	69.223655
1036.103862	-8.961909	69.228660
1035.416699	2.313404	69.233665
1034.581653	-7.221628	69.238670
1033.887381	-17.318344	69.243674
1033.115670	13.241595	69.248679
1032.952428	-8.666944	69.253684
1031.826285	-6.898248	69.258689
1031.028385	7.088013	69.263694
1030.828930	-8.800501	69.268698
1030.302819	16.977092	69.273703
1029.349007	-5.493207	69.278708
1028.831455	-5.043418	69.283713
1028.071160	0.224543	69.288718
1027.785309	-2.861647	69.293722
1026.600908	-1.183024	69.298727
1025.656002	2.468034	69.303732
1025.752100	-3.637165	69.308737
1024.821053	-4.900325	69.313742
1024.323576	-4.540457	69.318746
1023.931317	8.299529	69.323751
1022.730028	-8.903996	69.328756
1022.031627	-5.232233	69.333761
1021.030283	6.685979	69.338766
1020.921824	-14.729812	69.343770
1020.349090	13.729595	69.348775
1019.270291	0.808335	69.353780
1018.716208	-14.438726	69.358785
1017.835759	18.385589	69.363790
1018.002749	-8.574230	69.368794
1016.674681	2.539708	69.373799
1015.888629	15.401349	69.378804
1015.875774	-19.161992	69.383809
1014.787095	15.710707	69.388814
1014.077486	-5.618918	69.393818
1013.233546	-5.807877	69.398823
1012.915984	6.432043	69.403828
1012.445170	-3.864221	69.408833
1011.411077	-8.994860	69.413838
1010.710710	10.108666	69.418842
1010.356552	-26.683693	69.423847
1009.460741	10.329682	69.428852
1009.169061	-3.030595	69.433857
1007.654854	2.128665	69.438862
1007.497085	-27.404971	69.443866
1006.842543	18.127808	69.448871
1006.330227	-18.283031	69.453876
1006.366728	2.827321	69.458881
1005.014310	-19.473874	69.463886
1004.503446	-1.195263	69.468890
1003.812831	-3.614681	69.473895
1002.438414	-11.712489	69.478900
1002.461580	-14.294349	69.483905
1001.652219	11.132497	69.488910
1000.722776	-13.948249	69.493914
999.775004	-16.814009	69.498919
999.296470	1.350656	69.503924
999.247680	-21.418122	69.508929
998.610342	17.269802	69.513934
998.157724	-5.062607	69.518938
997.040939	-18.274249	69.523943
996.320867	4.831394	69.528948
996.100379	-13.728165	69.533953
994.787431	-1.091776	69.538958
994.007064	5.201212	69.543962
993.639309	-3.501438	69.548967
992.918331	-3.725723	69.553972
992.217383	-6.473062	69.558977
991.286780	9.866540	69.563982
991.236171	-23.739908	69.568986
990.652227	13.849882	69.573991
989.912956	-18.598378	69.578996
988.943208	0.820797	69.584001
988.492252	-14.707577	69.589006
987.933707	1.725781	69.594010
987.046101	-13.037714	69.599015
986.189396	-0.431335	69.604020
985.810240	-2.335775	69.609025
985.367079	-4.933324	69.614030
984.638936	4.528789	69.619034
983.715246	1.200325	69.624039
983.201453	3.018266	69.629044
982.948468	-6.450086	69.634049
982.076539	3.916385	69.639054
981.284984	-1.782666	69.644058
980.781649	5.220001	69.649063
979.597842	-0.181684	69.654068
979.149505	3.240579	69.659073
978.214474	-8.809427	69.664078
977.886826	-4.657347	69.669082
977.338520	-2.436538	69.674087
975.986988	0.940201	69.679092
976.070712	-9.955191	69.684097
975.466946	-15.794494	69.689102
974.629708	11.931161	69.694106
973.811245	-7.946151	69.699111
973.074801	-9.301751	69.704116
972.933149	-0.137950	69.709121
971.957935	-16.142699	69.714126
971.091583	15.550314	69.719130
970.524876	10.460436	69.724135
970.183800	-18.788581	69.729140
969.363719	7.095685	69.734145
967.809435	1.330346	69.739150
967.834962	-21.524362	69.744154
967.427511	-7.059356	69.749159
966.687951	-3.641217	69.754164
966.229875	-29.900735	69.759169
964.978076	9.810563	69.764174
964.411472	-8.995108	69.769178
964.266706	-21.678594	69.774183
963.504987	10.395135	69.779188
962.586260	-20.630578	69.784193
962.046544	3.897103	69.789198
961.974991	-5.988028	69.794202
960.511165	8.304468	69.799207
960.358320	-0.165877	69.804212
959.300969	-9.011094	69.809217
958.148836	3.393153	69.814222
957.394862	-25.042702	69.819226
957.257158	-1.443130	69.824231
956.837278	7.181496	69.829236
956.580492	-23.027051	69.834241
955.351018	0.293674	69.839246
954.668912	7.610208	69.844250
954.178749	3.455868	69.849255
953.623632	-9.816742	69.854260
953.060409	-5.242416	69.859265
951.939805	0.259505	69.864270
951.609208	-21.925123	69.869274
950.853884	20.340608	69.874279
949.807714	-10.895065	69.879284
949.524976	-9.176960	69.884289
948.743692	-3.574495	69.889294
948.413601	0.677322	69.894298
947.371046	-16.229716	69.899303
946.540647	7.569972	69.904308
945.890051	-3.744721	69.909313
945.802344	-25.600574	69.914318
945.044480	25.504023	69.919322
944.171235	-9.354477	69.924327
943.427743	3.919847	69.929332
942.972340	-22.557709	69.934337
941.704030	12.206378	69.939342
941.682196	-1.925344	69.944346
941.188154	-14.963245	69.949351
940.143821	1.807599	69.954356
939.449578	-10.067820	69.959361
938.562747	16.500416	69.964366
938.780507	-3.473962	69.969370
937.917654	-10.139319	69.974375
936.615515	-8.708416	69.979380
936.211219	9.149567	69.984385
935.311232	-11.671917	69.989390
935.070061	6.825552	69.994394
934.002164	-14.782884	69.999399
933.431772	-7.875198	70.004404
933.295246	2.232343	70.009409
932.570148	-18.452963	70.014414
931.576308	13.364406	70.019418
930.995388	-7.632428	70.024423
930.038582	7.019352	70.029428
930.138852	-14.155249	70.034433
928.579797	-5.830308	70.039438
928.180321	5.377169	70.044442
927.980449	5.807965	70.049447
926.889229	2.939827	70.054452
926.397974	-0.025357	70.059457
925.595962	-15.338580	70.064462
925.185146	3.177995	70.069466
924.406763	-8.997832	70.074471
923.276568	3.360359	70.079476
922.868712	-20.287934	70.084481
922.244097	17.562202	70.089486
922.220296	-28.802356	70.094490
921.344508	12.096433	70.099495
920.167892	-23.186807	70.104500
919.828842	1.542314	70.109505
919.548129	-6.510297	70.114510
918.391301	-9.345912	70.119514
917.725260	-0.141244	70.124519
916.956102	-4.604399	70.129524
916.382649	-2.835298	70.134529
915.391937	11.443433	70.139534
914.636947	-15.084217	70.144538
914.392836	16.571278	70.149543
913.766577	-20.261320	70.154548
913.551087	-12.197484	70.159553
912.558701	7.119663	70.164558
911.796427	-18.232037	70.169562
911.424516	3.181393	70.174567
910.449980	-3.286417	70.179572
909.709541	-0.539878	70.184577
908.888754	-10.113390	70.189582
908.398641	2.589205	70.194586
908.038407	9.412999	70.199591
907.055211	-3.048764	70.204596
906.607422	-1.949335	70.209601
906.348871	4.650126	70.214606
905.096736	-11.766242	70.219610
904.090233	8.645938	70.224615
903.677137	1.057498	70.229620
903.166355	-9.259176	70.234625
902.765999	13.276808	70.239630
902.264026	-23.972927	70.244634
901.344101	6.146974	70.249639
900.856354	-1.992534	70.254644
899.641428	5.601181	70.259649
898.852602	-23.270623	70.264654
898.697894	16.288184	70.269658
897.793805	-18.322510	70.274663
897.460545	18.718047	70.279668
896.835877	1.839130	70.284673
896.139314	3.701941	70.289678
895.454075	2.003914	70.294682
894.682155	5.624334	70.299687
893.907405	-3.757814	70.304692
893.348533	5.716800	70.309697
892.789964	-16.149272	70.314702
891.781869	10.517098	70.319706
891.083152	-10.260702	70.324711
890.227789	9.868820	70.329716
890.459124	-12.868831	70.334721
889.337584	-11.963364	70.339726
888.384768	7.584024	70.344730
887.877532	-11.724624	70.349735
887.127463	-4.083467	70.354740
887.237821	-16.492166	70.359745
886.200866	7.017135	70.364750
885.148471	-5.367372	70.369754
885.002520	2.411027	70.374759
883.865800	-0.793611	70.379764
883.343248	-15.400689	70.384769
882.331640	1.869564	70.389774
882.063816	0.352684	70.394778
881.923274	-5.000520	70.399783
880.636106	-8.761506	70.404788
880.299952	3.074532	70.409793
879.492392	2.763139	70.414798
878.884898	-4.184099	70.419802
877.901988	10.419812	70.424807
877.113626	-14.016282	70.429812
876.697875	1.076077	70.434817
876.614422	0.647869	70.439822
875.597270	-5.724837	70.444826
874.836274	0.044722	70.449831
874.659325	-19.313321	70.454836
873.628067	3.121210	70.459841
872.324525	-9.064051	70.464846
872.334418	-5.154908	70.469850
871.742720	-3.868575	70.474855
870.732078	13.303773	70.479860
870.249285	-2.172199	70.484865
869.207777	-11.098733	70.489870
869.122625	15.761370	70.494874
867.952199	-10.288576	70.499879
867.231445	-11.075808	70.504884
866.705595	21.411390	70.509889
865.841535	16.655856	70.514894
865.998661	-8.581971	70.519898
865.341464	1.815003	70.524903
864.100643	-21.284398	70.529908
863.763564	13.012963	70.534913
863.069243	-14.203952	70.539918
861.993369	6.790106	70.544922
861.578206	-4.878977	70.549927
860.947580	-6.300269	70.554932
860.634257	-11.692198	70.559937
859.886881	3.211678	70.564942
859.205126	-18.308354	70.569946
858.186145	0.522616	70.574951
857.276406	-6.579929	70.579956
856.751915	-13.150874	70.584961
855.944880	10.657720	70.589966
855.782195	-12.979116	70.594970
855.288909	6.053611	70.599975
854.576127	-1.769381	70.604980
853.981057	-8.843161	70.609985
853.395244	2.174785	70.614990
852.436021	-1.540614	70.619994
851.536642	-11.929458	70.624999
850.739043	-4.842100	70.630004
850.481611	-9.659476	70.635009
849.471887	6.360019	70.640014
848.544405	-16.998974	70.645018
848.167503	-3.823988	70.650023
847.712039	4.875691	70.655028
847.650987	-10.938612	70.660033
846.660969	-1.280263	70.665038
845.558569	2.052160	70.670042
845.080211	-18.770138	70.675047
844.571622	8.685596	70.680052
843.809278	0.704921	70.685057
843.178285	-3.739199	70.690062
842.661956	4.577522	70.695066
841.614149	-1.891211	70.700071
840.796534	1.031627	70.705076
840.392154	-13.289906	70.710081
839.590424	13.741004	70.715086
839.492574	-6.828069	70.720090
838.546341	-16.490386	70.725095
837.642987	8.923037	70.730100
837.565143	-19.724442	70.735105
836.366202	-10.794479	70.740110
835.447288	-7.477067	70.745114
835.081738	-12.684067	70.750119
834.183009	13.167002	70.755124
834.399934	-15.043297	70.760129
833.572430	-3.245749	70.765134
832.748845	-17.137870	70.770138
832.438289	7.957283	70.775143
830.874758	-11.052336	70.780148
830.498031	-7.950523	70.785153
829.766043	-7.466563	70.790158
829.202211	12.391074	70.795162
828.777508	-16.776765	70.800167
827.597756	6.417819	70.805172
827.184486	-6.721213	70.810177
826.670942	-3.767926	70.815182
826.206645	8.545810	70.820186
825.504770	-9.394634	70.825191
824.548537	-2.521707	70.830196
824.316921	7.957343	70.835201
822.942313	-13.137021	70.840206
822.405675	11.248254	70.845210
822.004823	-8.334337	70.850215
821.543613	-8.082700	70.855220
820.963405	-0.408642	70.860225
819.801038	2.722034	70.865230
819.082934	-17.743563	70.870234
819.109796	4.902588	70.875239
817.676947	-18.008529	70.880244
817.002421	5.413130	70.885249
816.693833	-6.996692	70.890254
816.078147	1.367383	70.895258
815.582252	-2.598360	70.900263
814.468922	-10.721838	70.905268
813.844595	9.515991	70.910273
813.464536	-14.366915	70.915278
813.062462	11.160682	70.920282
812.462487	-11.662247	70.925287
811.432932	1.492054	70.930292
811.384386	-9.782800	70.935297
809.921743	12.573770	70.940302
809.158712	-23.700838	70.945306
808.953966	6.606415	70.950311
808.132401	-15.055338	70.955316
807.459703	3.198577	70.960321
806.465066	-4.395037	70.965326
805.716816	11.046712	70.970330
805.516196	-24.155247	70.975335
805.294015	16.524391	70.980340
804.550290	-29.205137	70.985345
803.342496	18.274800	70.990350
802.798430	-23.755606	70.995354
802.041502	11.039054	71.000359
801.273799	0.432155	71.005364
801.089013	11.625966	71.010369
800.404142	2.693150	71.015374
799.313000	-9.227841	71.020378
798.640347	12.727030	71.025383
797.946044	3.289535	71.030388
797.793903	-10.280541	71.035393
797.117032	-9.086286	71.040398
796.259553	15.137186	71.045402
795.826375	-19.545234	71.050407
795.024616	11.624999	71.055412
794.095443	-12.298223	71.060417
793.440881	8.210911	71.065422
792.836308	-13.684063	71.070426
792.685770	-11.154392	71.075431
791.381640	2.199733	71.080436
790.552671	-6.845748	71.085441
790.277006	-3.613366	71.090446
789.942091	-11.840239	71.095450
788.902737	-8.273415	71.100455
788.020039	1.151836	71.105460
787.497559	-9.289090	71.110465
787.055265	-23.940437	71.115470
786.521967	25.223494	71.120474
785.628573	-3.440829	71.125479
785.346730	-34.039510	71.130484
784.446864	7.605795	71.135489
783.154676	5.452506	71.140494
782.690151	-26.107396	71.145498
782.086939	4.327926	71.150503
781.808966	-21.012481	71.155508
781.596767	4.595257	71.160513
780.200498	-6.469788	71.165518
779.611574	-1.369390	71.170522
779.089616	4.731133	71.175527
778.707082	-18.949515	71.180532
777.837353	-5.618813	71.185537
776.452124	9.853376	71.190542
776.446649	-16.046057	71.195546
776.237439	-15.940178	71.200551
774.874800	4.831473	71.205556
774.657689	-18.884969	71.210561
773.888877	-0.417069	71.215566
772.923794	-21.551342	71.220570
771.990236	2.138618	71.225575
771.717610	-27.567443	71.230580
771.586888	6.692299	71.235585
770.493550	-18.827380	71.240590
770.020608	-15.345985	71.245594
769.323225	-5.079794	71.250599
768.781418	-30.564252	71.255604
767.907156	15.651534	71.260609
767.270327	-9.034121	71.265614
766.502147	-11.209316	71.270618
765.337790	-1.884298	71.275623
764.587321	-16.067135	71.280628
764.463865	-2.681770	71.285633
763.778420	-12.929593	71.290638
763.277572	8.182672	71.295642
763.032324	-11.136093	71.300647
761.686810	-11.174161	71.305652
761.395384	9.855885	71.310657
760.691530	-2.098359	71.315662
760.123505	2.322233	71.320666
758.975004	-2.421086	71.325671
758.563550	0.527000	71.330676
758.158304	-5.928868	71.335681
756.954567	-1.011278	71.340686
756.426172	-1.070618	71.345690
756.255297	-7.163268	71.350695
755.517611	-4.841309	71.355700
754.472418	-0.666439	71.360705
753.529205	6.988154	71.365710
753.176742	3.272392	71.370714
752.853253	-4.845914	71.375719
751.987208	5.620595	71.380724
750.993911	5.259967	71.385729
750.669939	1.583823	71.390734
750.318172	0.528158	71.395738
749.473605	-0.542092	71.400743
748.384369	11.196231	71.405748
748.172915	-6.211998	71.410753
747.734575	6.666863	71.415758
746.751088	6.299944	71.420762
745.806417	-4.736052	71.425767
745.406104	-2.563989	71.430772
745.047379	-4.164147	71.435777
743.856367	-2.306157	71.440782
743.343219	-8.110935	71.445786
743.077433	-14.765610	71.450791
741.505414	2.882461	71.455796
740.983036	-8.670171	71.460801
740.294351	-1.485012	71.465806
740.243683	-13.201042	71.470810
740.015990	-4.750501	71.475815
738.935300	-2.143705	71.480820
738.321712	-9.998210	71.485825
737.475366	2.847835	71.490830
736.659910	-10.121485	71.495834
735.819813	-4.258880	71.500839
735.025098	-4.212742	71.505844
734.562417	1.184520	71.510849
734.310026	2.645514	71.515854
733.882939	-6.394541	71.520858
733.034117	-3.327938	71.525863
732.212410	3.086806	71.530868
731.936175	-9.914744	71.535873
730.446661	3.853678	71.540878
729.848652	0.836152	71.545882
729.419064	-5.626874	71.550887
729.004934	-13.295519	71.555892
728.452359	4.936125	71.560897
727.540357	-3.575739	71.565902
727.141154	-10.406282	71.570906
726.578630	-6.704045	71.575911
725.251461	-6.838050	71.580916
724.744935	-6.527144	71.585921
724.485623	-4.424833	71.590926
723.621337	-8.688278	71.595930
722.981439	-13.591391	71.600935
722.052427	-4.910928	71.605940
721.983672	-12.655058	71.610945
720.672636	-1.381297	71.615950
720.144170	-4.819881	71.620954
719.447730	-6.700568	71.625959
718.933609	-3.485408	71.630964
718.598901	-6.817651	71.635969
717.654406	-10.417069	71.640974
717.068478	-5.741321	71.645978
716.421686	-1.385449	71.650983
715.242551	0.134787	71.655988
714.844655	4.952484	71.660993
714.096552	4.891864	71.665998
713.779546	-3.035087	71.671002
713.287984	-6.823306	71.676007
712.052970	2.905628	71.681012
711.620612	-0.505682	71.686017
710.862689	4.468679	71.691022
710.578232	0.292686	71.696026
709.709180	-0.314777	71.701031
708.785449	-11.836610	71.706036
708.442835	-14.256152	71.711041
707.835086	8.737008	71.716046
707.122479	-0.629729	71.721050
706.655924	-4.024554	71.726055
705.692401	2.829073	71.731060
705.138053	1.682672	71.736065
704.133005	-11.194948	71.741070
703.386487	7.408185	71.746074
703.376450	3.245269	71.751079
702.548240	0.046791	71.756084
701.708339	-2.703567	71.761089
700.828705	4.172975	71.766094
700.133632	7.776481	71.771098
700.130295	4.564936	71.776103
699.531255	-4.088203	71.781108
698.572758	-9.708526	71.786113
698.088453	0.266722	71.791118
697.105643	1.891321	71.796122
696.235902	4.926575	71.801127
695.571693	1.279383	71.806132
695.531109	-10.881352	71.811137
694.445135	-0.960111	71.816142
693.738025	6.125496	71.821146
693.351530	7.335045	71.826151
692.443499	7.973225	71.831156
692.022974	-4.636355	71.836161
690.994900	3.954243	71.841166
690.309164	-13.914586	71.846170
690.173630	5.529510	71.851175
689.308410	3.016566	71.856180
688.647083	-3.710737	71.861185
688.078812	0.307801	71.866190
687.382265	-3.624386	71.871194
686.611989	14.104216	71.876199
685.682768	-8.593695	71.881204
685.576611	-4.047944	71.886209
684.823217	1.688913	71.891214
683.769735	5.683788	71.896218
683.289955	-5.919761	71.901223
682.717985	6.204551	71.906228
681.828780	-10.469717	71.911233
680.695097	2.824196	71.916238
679.992819	-7.170194	71.921242
680.186438	-0.410923	71.926247
679.564200	6.482986	71.931252
679.175956	-1.932487	71.936257
678.233261	-0.435689	71.941262
677.293886	-0.257694	71.946266
677.064147	4.049128	71.951271
675.581763	-3.171884	71.956276
675.447814	-10.779478	71.961281
674.354707	2.793392	71.966286
674.238244	10.633323	71.971290
673.424404	-7.897900	71.976295
672.417419	4.724591	71.981300
671.977886	-6.123729	71.986305
671.866428	-4.629980	71.991310
670.695286	-2.292593	71.996314
669.843975	-2.253191	72.001319
669.270748	13.094479	72.006324
668.979177	-8.538059	72.011329
667.795428	5.538082	72.016334
667.163452	3.837948	72.021338
666.717194	-6.662384	72.026343
666.012317	2.195289	72.031348
666.078659	9.353281	72.036353
665.169763	-5.685773	72.041358
664.009840	-0.524395	72.046362
663.609460	-1.583344	72.051367
662.360375	3.019825	72.056372
661.929688	-3.914498	72.061377
661.124368	5.462197	72.066382
661.003048	-1.522965	72.071386
660.351977	-8.776992	72.076391
659.124546	-2.403278	72.081396
658.917494	-0.356589	72.086401
658.438225	-0.264466	72.091406
657.954600	-8.371442	72.096410
657.055586	-12.399105	72.101415
655.731874	-5.630031	72.106420
655.670606	-9.863628	72.111425
654.325356	2.426393	72.116430
653.841268	-2.488898	72.121434
653.521157	-3.024487	72.126439
652.904321	3.269349	72.131444
652.657822	5.901037	72.136449
652.134419	8.764467	72.141454
650.981686	9.369091	72.146458
650.433382	-0.593043	72.151463
649.213299	2.184213	72.156468
648.710766	-3.120783	72.161473
648.182695	3.139997	72.166478
647.847345	-1.417372	72.171482
647.172647	-1.139592	72.176487
646.016836	-4.440417	72.181492
645.572681	-5.686349	72.186497
645.126985	-5.828217	72.191502
644.649540	-8.424967	72.196506
644.011107	-2.643333	72.201511
643.263406	-1.481911	72.206516
642.243712	-2.557350	72.211521
641.682674	-5.501895	72.216526
640.926482	1.145279	72.221530
640.626741	-0.610906	72.226535
639.276329	-4.937250	72.231540
638.774855	3.008138	72.236545
638.093797	-5.505769	72.241550
638.105772	-3.550725	72.246554
637.300636	-11.502421	72.251559
635.694078	2.380870	72.256564
635.548313	-6.989372	72.261569
635.053691	2.926028	72.266574
634.570474	2.963594	72.271578
634.151078	-3.677643	72.276583
633.140797	4.517496	72.281588
632.670983	-8.342821	72.286593
631.557078	-2.195323	72.291598
630.499387	0.179206	72.296602
630.681338	-6.321257	72.301607
629.338346	0.458786	72.306612
629.567230	-1.936640	72.311617
628.476292	-0.953934	72.316622
627.555601	1.034519	72.321626
627.320610	-6.301525	72.326631
626.609655	-1.487582	72.331636
625.909755	-7.253129	72.336641
624.590892	-7.367903	72.341646
624.416868	1.435201	72.346650
624.373758	4.237919	72.351655
623.224102	17.804054	72.356660
622.648285	-0.850207	72.361665
622.151224	-0.731591	72.366670
621.137704	5.109782	72.371674
620.049666	-0.663337	72.376679
619.327124	-5.360881	72.381684
619.338553	-8.745074	72.386689
618.911630	-6.374801	72.391694
618.105405	1.062480	72.396698
617.180651	-3.013107	72.401703
616.420575	1.095910	72.406708
616.394872	-1.511276	72.411713
615.149649	-3.326614	72.416718
614.388535	3.605190	72.421722
613.969901	-2.859553	72.426727
613.185926	1.732644	72.431732
612.396176	-7.109280	72.436737
611.732656	-0.073176	72.441742
611.349335	5.314619	72.446746
611.078496	-13.008161	72.451751
609.638009	7.402222	72.456756
608.975258	-0.267806	72.461761
608.378862	-7.372834	72.466766
608.064431	-7.720096	72.471770
607.866627	0.159588	72.476775
607.040213	4.998232	72.481780
606.337474	-3.707745	72.486785
605.062903	-6.530762	72.491790
604.242576	-1.026068	72.496794
603.693051	-6.377181	72.501799
603.078605	-5.823570	72.506804
603.098739	-7.605460	72.511809
602.241771	-0.809771	72.516814
601.428594	-3.646345	72.521818
600.860114	-1.218833	72.526823
600.230297	-0.781039	72.531828
599.522478	-11.596067	72.536833
598.795039	-3.775535	72.541838
597.941237	-2.967770	72.546842
597.489516	-6.068478	72.551847
596.407752	-0.097964	72.556852
596.221551	-7.309314	72.561857
595.567468	-7.053727	72.566862
594.993017	-7.868909	72.571866
594.163345	-7.836081	72.576871
593.066219	0.494319	72.581876
593.058545	-8.465841	72.586881
591.818131	-2.446407	72.591886
590.953662	3.495812	72.596890
590.465742	4.737297	72.601895
590.088258	1.370887	72.606900
589.750575	-10.523329	72.611905
589.253336	1.145983	72.616910
588.437897	-3.074729	72.621914
587.959117	1.588711	72.626919
586.845956	4.706920	72.631924
586.092116	4.558947	72.636929
585.424820	-5.907735	72.641934
584.879150	0.273857	72.646938
584.519199	8.579897	72.651943
583.513526	-14.294991	72.656948
582.884771	1.916185	72.661953
582.342812	2.491372	72.666958
581.478940	-7.169751	72.671962
580.669268	-10.194523	72.676967
580.111788	4.048395	72.681972
579.947826	-9.702671	72.686977
578.853302	3.488847	72.691982
577.984921	-12.865418	72.696986
577.373229	-17.539598	72.701991
576.952801	6.008745	72.706996
576.304070	-0.469804	72.712001
575.508357	-6.108115	72.717006
574.792487	-9.455317	72.722010
574.384104	0.783805	72.727015
573.867274	16.336958	72.732020
573.117495	-7.108523	72.737025
572.120897	8.164657	72.742030
571.761911	-2.195015	72.747034
571.221094	-6.979829	72.752039
569.954596	-4.272413	72.757044
569.476091	6.238067	72.762049
568.554961	2.111461	72.767054
568.620637	-2.125004	72.772058
567.736678	-10.795791	72.777063
566.565431	-1.993129	72.782068
566.149271	-5.815398	72.787073
566.072302	-14.540598	72.792078
565.596419	-1.819755	72.797082
564.409376	-4.797034	72.802087
563.732505	6.804705	72.807092
563.351059	3.394778	72.812097
562.181406	-6.181367	72.817102
561.661686	-10.827617	72.822106
560.864488	-0.526569	72.827111
560.523469	-2.321897	72.832116
559.993537	-9.972058	72.837121
559.264094	-0.023983	72.842126
558.453926	-3.324625	72.847130
557.977459	-8.165413	72.852135
556.935505	-0.411465	72.857140
556.529099	-2.945398	72.862145
556.028001	-7.427465	72.867150
555.103627	2.129055	72.872154
554.589134	-3.002132	72.877159
553.655149	-1.050957	72.882164
553.203978	-3.525722	72.887169
552.265599	2.633274	72.892174
551.128064	1.229728	72.897178
551.084024	-4.381647	72.902183
550.676726	1.856756	72.907188
550.214190	-11.726903	72.912193
549.484369	0.107183	72.917198
548.507660	-2.165609	72.922202
548.233296	-8.782616	72.927207
547.212914	8.301464	72.932212
546.618902	-3.228658	72.937217
545.913331	0.236212	72.942222
545.031134	-4.713407	72.947226
544.298364	-8.086292	72.952231
543.132887	7.073451	72.957236
542.857786	-11.966111	72.962241
542.406795	3.827267	72.967246
542.027497	3.416232	72.972250
542.009149	-10.310711	72.977255
540.489210	3.442142	72.982260
540.065852	-5.369807	72.987265
539.758864	-1.962114	72.992270
538.784703	-0.594288	72.997274
538.025580	0.280414	73.002279
537.399329	6.854880	73.007284
536.406457	-18.850935	73.012289
535.583026	-1.845541	73.017294
534.973373	-3.151820	73.022298
534.690082	-2.362370	73.027303
534.317733	2.750883	73.032308
533.713982	-6.256247	73.037313
532.713289	-12.677136	73.042318
532.179266	-4.102112	73.047322
531.502946	-14.037498	73.052327
530.071997	-1.863084	73.057332
529.785281	-2.030255	73.062337
529.443379	-9.759240	73.067342
529.082441	7.658177	73.072346
528.373381	-6.862302	73.077351
527.582865	-6.386278	73.082356
527.050908	-0.911727	73.087361
525.635067	6.925443	73.092366
524.699178	0.978332	73.097370
524.458670	-6.344201	73.102375
523.704188	1.174743	73.107380
523.555484	8.770655	73.112385
523.531912	-5.660324	73.117390
522.606327	-16.107909	73.122394
521.923864	14.139767	73.127399
520.564555	-0.759663	73.132404
519.743683	-8.431275	73.137409
518.798979	0.273823	73.142414
518.462026	-1.358151	73.147418
518.670349	0.008974	73.152423
518.069823	-0.223321	73.157428
517.014122	-17.987402	73.162433
516.453778	-7.632618	73.167438
515.612614	11.785092	73.172442
514.860379	1.190042	73.177447
514.209279	1.225989	73.182452
513.793345	-10.081757	73.187457
512.333628	2.846268	73.192462
511.794283	-0.106430	73.197466
511.301282	-1.817620	73.202471
511.175691	4.043192	73.207476
510.778569	-12.345106	73.212481
509.151057	13.401313	73.217486
508.833529	-1.610443	73.222490
508.757346	-2.848735	73.227495
507.457899	-2.296366	73.232500
506.670518	12.096722	73.237505
506.150773	2.890142	73.242510
505.951763	-5.659504	73.247514
505.287481	2.094223	73.252519
504.221482	-4.838201	73.257524
503.753964	-2.000995	73.262529
503.159892	2.873203	73.267534
501.783527	-1.906222	73.272538
501.266751	-5.728219	73.277543
500.570538	17.181277	73.282548
500.377156	-12.201443	73.287553
499.907290	-11.945216	73.292558
499.214109	6.379792	73.297562
498.765676	-2.424999	73.302567
497.864643	-5.463573	73.307572
496.773043	6.773494	73.312577
496.443894	-0.438726	73.317582
495.428519	-7.593664	73.322586
495.332619	19.821543	73.327591
494.400270	8.834161	73.332596
493.341261	8.689099	73.337601
492.721147	-13.428748	73.342606
492.214985	23.385372	73.347610
492.298289	-15.004417	73.352615
490.980251	10.265369	73.357620
490.288709	-10.776707	73.362625
489.955423	-12.928053	73.367630
489.117339	2.070742	73.372634
488.431390	-4.026548	73.377639
487.494131	13.440106	73.382644
487.411717	-14.060140	73.387649
486.361984	-6.005325	73.392654
485.268260	-6.420807	73.397658
485.161603	-8.272380	73.402663
484.773767	4.500675	73.407668
484.305977	-8.159652	73.412673
483.321881	-18.222598	73.417678
482.504873	-0.604812	73.422682
482.060242	-6.463012	73.427687
480.898749	3.476640	73.432692
480.459331	-4.113806	73.437697
480.023044	-10.287132	73.442702
478.808584	-3.822373	73.447706
478.047950	3.552489	73.452711
477.412980	-5.798139	73.457716
476.935449	-23.365725	73.462721
476.639001	4.936066	73.467726
476.203825	-5.364134	73.472730
475.635461	-4.770527	73.477735
474.846538	-2.539673	73.482740
474.242678	-14.664251	73.487745
472.996849	2.458907	73.492750
472.302074	-9.845147	73.497754
472.095397	-15.320222	73.502759
471.453519	-0.614446	73.507764
470.731881	-4.225612	73.512769
469.847813	3.036458	73.517774
469.157236	-8.214909	73.522778
468.690800	-10.524804	73.527783
467.432749	-5.595285	73.532788
467.013288	-22.416794	73.537793
466.491251	2.874402	73.542798
466.551875	-19.642016	73.547802
465.624632	-2.340968	73.552807
464.698213	-4.754194	73.557812
464.123889	-14.759416	73.562817
463.186617	-5.637617	73.567822
462.200196	1.606068	73.572826
461.864326	-10.069216	73.577831
461.199510	-7.333030	73.582836
460.972180	-17.202728	73.587841
459.886685	3.479138	73.592846
459.051688	-6.850396	73.597850
458.755932	-0.476798	73.602855
458.301335	8.886644	73.607860
457.390395	-11.975387	73.612865
456.887958	-5.240873	73.617870
456.103332	-13.047534	73.622874
455.981441	-1.633546	73.627879
454.583986	0.421462	73.632884
453.827490	-24.123516	73.637889
453.423719	1.845815	73.642894
452.932077	-18.837011	73.647898
451.912429	5.617300	73.652903
450.990862	-18.778391	73.657908
450.596044	-10.055234	73.662913
450.464612	2.276443	73.667918
449.598848	-8.139644	73.672922
448.978906	-21.581492	73.677927
448.177102	9.024210	73.682932
447.577123	-11.256605	73.687937
446.546021	-2.635490	73.692942
445.444455	-15.300477	73.697946
445.392353	-2.483150	73.702951
444.997026	-13.898231	73.707956
444.410835	6.521176	73.712961
443.566015	-20.792924	73.717966
442.519803	8.307953	73.722970
442.267906	-30.783696	73.727975
442.001031	15.619105	73.732980
441.220417	-19.064531	73.737985
440.369989	6.477675	73.742990
439.468981	1.540555	73.747994
438.378092	-14.901180	73.752999
437.949123	13.607806	73.758004
437.524677	-21.373829	73.763009
437.000813	4.393875	73.768014
436.522875	-6.175455	73.773018
435.782765	0.018216	73.778023
435.077836	-1.528311	73.783028
434.380031	-6.475725	73.788033
433.340638	1.318855	73.793038
432.969451	-3.521332	73.798042
432.676106	-24.108007	73.803047
431.880730	1.830677	73.808052
430.943978	-21.506066	73.813057
430.307636	-5.041378	73.818062
429.555643	-7.876599	73.823066
428.826375	-9.433438	73.828071
428.040733	-4.366288	73.833076
427.445960	-11.463631	73.838081
427.322459	-14.810550	73.843086
426.370262	-9.770479	73.848090
425.618492	-9.217022	73.853095
424.580092	3.331694	73.858100
424.449654	-14.122457	73.863105
423.900129	-13.419882	73.868110
422.799050	3.010057	73.873114
422.431497	-12.216031	73.878119
421.813393	6.224747	73.883124
421.425596	-5.409142	73.888129
420.326298	-1.495174	73.893134
419.353732	-3.683420	73.898138
419.223185	-0.035759	73.903143
418.256874	10.472036	73.908148
417.898763	-1.805223	73.913153
417.073343	-15.162289	73.918158
416.462164	0.210352	73.923162
416.019630	-3.563531	73.928167
414.987394	-1.472080	73.933172
414.163057	-21.367051	73.938177
413.920776	10.007325	73.943182
413.327613	-10.512670	73.948186
412.940676	-8.639147	73.953191
411.715882	-2.827118	73.958196
411.158282	-5.814726	73.963201
410.000389	-2.858044	73.968206
409.171650	-6.187209	73.973210
409.057002	-1.993328	73.978215
408.446594	-6.199333	73.983220
408.258997	7.579407	73.988225
407.763856	-3.848151	73.993230
406.828426	-6.766095	73.998234
406.125900	-3.104566	74.003239
404.781217	-12.507654	74.008244
403.782954	2.254916	74.013249
403.861337	-7.810137	74.018254
402.615175	-11.350319	74.023258
403.004126	-11.888471	74.028263
402.114519	-2.939821	74.033268
401.543958	-7.155326	74.038273
400.921802	-3.356799	74.043278
399.634699	-7.600051	74.048282
398.641405	-15.080140	74.053287
398.177705	2.227487	74.058292
397.708973	-7.304133	74.063297
397.589038	-4.930705	74.068302
396.820619	1.399944	74.073306
396.370566	-24.116303	74.078311
395.371996	-7.563937	74.083316
395.077996	-4.869474	74.088321
393.909431	-2.764176	74.093326
393.120606	0.051709	74.098330
392.884931	-5.609539	74.103335
392.020708	-9.171152	74.108340
391.612849	-8.737135	74.113345
390.956893	-9.045718	74.118350
389.923183	-4.426286	74.123354
389.356109	-6.458368	74.128359
388.371536	-4.879102	74.133364
387.905483	-6.108880	74.138369
387.413537	-5.027559	74.143374
386.860477	3.723978	74.148378
385.986942	-10.286123	74.153383
385.135262	-2.013684	74.158388
384.938924	-6.944797	74.163393
384.063190	-7.756073	74.168398
382.762197	11.755423	74.173402
383.035787	-11.010957	74.178407
382.480505	-2.557099	74.183412
381.714575	-3.557752	74.188417
380.712400	-18.301092	74.193422
380.036689	2.788555	74.198426
379.625091	-3.363453	74.203431
378.166727	-2.574393	74.208436
377.675381	-12.195436	74.213441
377.201239	-7.264638	74.218446
377.020212	-9.530111	74.223450
376.736519	-19.930101	74.228455
375.255288	3.247962	74.233460
374.790432	-23.107971	74.238465
374.283500	-11.555376	74.243470
373.736809	-12.371774	74.248474
372.781754	-11.035315	74.253479
371.875803	-2.863029	74.258484
371.299450	-5.488111	74.263489
371.013076	-1.960692	74.268494
370.098242	-4.926056	74.273498
369.788893	-3.504839	74.278503
368.773885	-8.510489	74.283508
368.475675	-14.117612	74.288513
367.630467	-5.636478	74.293518
367.089223	0.104494	74.298522
366.452730	-1.203771	74.303527
365.379758	0.430589	74.308532
364.848409	-1.424262	74.313537
364.370533	-0.611671	74.318542
363.729458	2.579629	74.323546
363.014575	-12.838662	74.328551
362.099624	1.686725	74.333556
361.929521	2.590615	74.338561
360.624116	-9.034220	74.343566
359.854794	5.139974	74.348570
359.397293	-5.202365	74.353575
358.724856	2.473844	74.358580
358.316063	-7.827371	74.363585
358.089128	-6.947540	74.368590
356.979632	2.137086	74.373594
356.282737	-6.024125	74.378599
355.962967	-2.300580	74.383604
355.126232	8.229157	74.388609
354.224408	5.408373	74.393614
353.550993	-0.161039	74.398618
353.485504	-16.236290	74.403623
352.236857	-9.138436	74.408628
351.517460	2.066425	74.413633
351.119082	-9.215688	74.418638
350.461469	-0.556293	74.423642
349.945133	3.234846	74.428647
348.872923	-4.696251	74.433652
348.468020	-7.310803	74.438657
347.913690	9.762129	74.443662
346.685311	-1.464989	74.448666
346.317710	-13.829010	74.453671
345.453095	4.581671	74.458676
345.337799	-11.077235	74.463681
344.663097	-10.936563	74.468686
343.347494	5.453473	74.473690
343.425220	-7.356816	74.478695
342.523838	4.037890	74.483700
341.696053	-9.938480	74.488705
340.893645	-8.219501	74.493710
339.878359	12.140569	74.498714
339.936927	-4.865898	74.503719
339.507201	-1.818656	74.508724
338.620465	-10.113600	74.513729
338.228690	12.953948	74.518734
337.426950	2.620740	74.523738
336.640202	-9.506183	74.528743
335.941083	-10.443354	74.533748
335.198672	1.313930	74.538753
334.440975	-3.133497	74.543758
333.613751	-4.349860	74.548762
333.087959	-10.737532	74.553767
332.339725	-11.050316	74.558772
331.980378	-7.561727	74.563777
331.256121	-2.360837	74.568782
330.593801	-28.253207	74.573786
330.488329	1.508261	74.578791
329.398872	-16.959919	74.583796
328.453430	-0.177889	74.588801
328.141604	-9.620957	74.593806
327.145800	-1.409109	74.598810
326.452049	-14.094867	74.603815
325.407197	-22.588515	74.608820
324.946364	-8.014082	74.613825
324.982432	-4.470241	74.618830
324.216881	-17.843108	74.623834
323.482341	-0.691008	74.628839
322.558396	-11.495133	74.633844
321.919826	-17.945247	74.638849
321.401627	-8.702550	74.643854
320.147449	7.233028	74.648858
319.673865	-21.587728	74.653863
318.856090	19.610838	74.658868
318.771498	-6.856160	74.663873
318.673495	-8.083081	74.668878
317.000836	10.864800	74.673882
316.932337	-6.767931	74.678887
315.855776	18.135438	74.683892
315.805301	-26.805361	74.688897
314.621471	5.638353	74.693902
313.718975	-20.348201	74.698906
313.527648	1.734948	74.703911
313.021246	-9.307598	74.708916
311.851183	-11.216753	74.713921
310.961542	2.394754	74.718926
310.838916	-7.029582	74.723930
310.634495	-10.614318	74.728935
309.350752	-10.006005	74.733940
308.832904	-2.452193	74.738945
308.171329	-31.758601	74.743950
307.626515	-4.251444	74.748954
306.850535	-9.049167	74.753959
306.520400	-9.122663	74.758964
305.903232	-8.518086	74.763969
304.750295	-5.529034	74.768974
304.188563	-8.951174	74.773978
303.617677	-29.250724	74.778983
302.375496	4.432251	74.783988
301.800947	-9.076706	74.788993
301.851994	-18.397832	74.793998
300.989879	-3.339990	74.799002
299.900529	-16.678587	74.804007
298.993246	9.024074	74.809012
298.422661	-15.388040	74.814017
298.053968	3.631125	74.819022
297.725910	-10.626709	74.824026
297.492166	3.187757	74.829031
296.765619	-1.387619	74.834036
295.866088	-11.998512	74.839041
294.651563	4.488965	74.844046
293.779408	-8.218810	74.849050
293.696121	-0.964479	74.854055
293.036150	-14.133399	74.859060
291.966443	4.363590	74.864065
291.305317	-18.111871	74.869070
290.571109	-7.338287	74.874074
290.612008	3.630297	74.879079
289.759493	-16.655917	74.884084
288.854376	7.097378	74.889089
288.301512	-8.428704	74.894094
287.757460	11.895691	74.899098
287.566385	-4.476496	74.904103
286.067763	-19.867596	74.909108
285.532304	12.047041	74.914113
285.387664	-20.560175	74.919118
284.121830	16.009126	74.924122
283.529006	-34.870443	74.929127
283.005193	5.242066	74.934132
282.880397	10.214969	74.939137
281.301853	-15.596016	74.944142
280.652202	8.577012	74.949146
280.342237	-30.566793	74.954151
280.157023	3.231555	74.959156
279.169703	-16.854979	74.964161
278.194571	-11.122109	74.969166
277.612862	-3.780455	74.974170
277.464965	-17.910880	74.979175
275.984425	21.873215	74.984180
275.390292	-12.206136	74.989185
274.991113	-10.852589	74.994190
274.458130	11.228256	74.999194
274.401069	-27.385034	75.004199
273.110899	16.698802	75.009204
271.977456	-6.956581	75.014209
271.863545	-24.608848	75.019214
271.046691	-2.818653	75.024218
270.476229	10.893377	75.029223
269.438197	-9.718062	75.034228
269.223503	-12.397607	75.039233
269.017325	8.913668	75.044238
267.415157	-11.592082	75.049242
267.471835	-8.557707	75.054247
266.426907	-10.076796	75.059252
265.946995	-4.411816	75.064257
265.208904	-15.825823	75.069262
264.443826	12.424486	75.074266
264.366288	-33.273586	75.079271
263.006473	11.955109	75.084276
262.400994	-28.205983	75.089281
262.048115	13.727395	75.094286
261.069712	-7.365034	75.099290
260.874215	-40.337808	75.104295
259.852493	12.825437	75.109300
259.237008	-21.990034	75.114305
258.738296	-2.555937	75.119310
257.321359	12.492598	75.124314
256.669584	-16.504727	75.129319
256.157069	-33.934179	75.134324
255.885419	-36.357070	75.139329
255.865966	-39.712669	75.144334
254.982205	-13.540732	75.149338
253.982656	17.161155	75.154343
253.476688	-12.632087	75.159348
252.709101	-22.284744	75.164353
251.630710	3.713254	75.169358
250.846170	-14.664716	75.174362
250.879767	7.344734	75.179367
250.232362	-11.009369	75.184372
249.102349	3.476210	75.189377
248.771480	-2.644482	75.194382
247.450998	21.343774	75.199386
247.873465	-22.060821	75.204391
246.783907	2.472461	75.209396
245.707728	11.666933	75.214401
245.840909	-31.144345	75.219406
244.726973	15.595234	75.224410
243.805864	-13.419079	75.229415
242.919744	-0.765285	75.234420
242.494635	3.140633	75.239425
242.648771	-8.719928	75.244430
241.289185	8.214871	75.249434
240.771042	-5.512781	75.254439
240.226610	-0.307420	75.259444
239.690340	3.600450	75.264449
238.399676	-10.078170	75.269454
237.876870	-4.430001	75.274458
237.644666	5.976590	75.279463
236.856077	-19.662236	75.284468
235.946723	-3.701188	75.289473
235.531217	15.194570	75.294478
234.436242	3.829564	75.299482
234.543022	-24.812431	75.304487
233.446624	-9.420785	75.309492
232.570625	19.966801	75.314497
231.945743	-0.410878	75.319502
231.754040	-20.619471	75.324506
231.052654	17.143438	75.329511
229.660762	0.838103	75.334516
229.441228	-30.058833	75.339521
229.074208	-3.458342	75.344526
228.270989	26.341835	75.349530
227.170582	-1.289370	75.354535
226.903475	-6.814700	75.359540
226.377795	13.092048	75.364545
225.889027	-8.173020	75.369550
225.063887	-33.641993	75.374554
224.739919	-45.208702	75.379559
223.364331	4.855596	75.384564
222.727555	7.484876	75.389569
222.150839	-12.041063	75.394574
221.715442	-33.011841	75.399578
221.148907	11.948481	75.404583
220.062177	-12.956879	75.409588
219.557572	-1.585976	75.414593
219.329226	4.251791	75.419598
218.333878	-0.512509	75.424602
217.721676	-24.015960	75.429607
217.037471	13.638549	75.434612
216.238827	-8.867003	75.439617
215.150807	7.579837	75.444622
214.383922	-21.233532	75.449626
214.260776	5.921003	75.454631
213.707086	17.943112	75.459636
213.259878	-10.902314	75.464641
213.230555	-28.795116	75.469646
211.966702	-8.947334	75.474650
210.646106	10.848023	75.479655
209.557391	-21.979225	75.484660
209.283637	-8.774955	75.489665
208.791507	-0.263335	75.494670
209.019931	-33.778319	75.499674
208.184512	-0.488176	75.504679
206.977211	-6.024464	75.509684
205.952849	3.814582	75.514689
206.598175	-38.195252	75.519694
204.867930	8.685127	75.524698
204.173834	19.632115	75.529703
203.411970	11.580652	75.534708
202.881196	-8.591241	75.539713
203.396756	-29.771959	75.544718
201.781294	23.936953	75.549722
201.223084	-13.653475	75.554727
200.555890	-26.229867	75.559732
199.385342	14.668534	75.564737
198.869228	-9.253930	75.569742
197.906905	-1.137260	75.574746
198.335881	-26.358326	75.579751
197.292190	-28.919893	75.584756
196.646038	16.374810	75.589761
196.223612	7.837175	75.594766
195.092805	-4.047189	75.599770
194.415983	-3.217043	75.604775
193.591436	-31.737347	75.609780
193.036709	-9.410231	75.614785
192.934868	-2.219176	75.619790
191.471007	-8.414686	75.624794
191.514294	-14.639163	75.629799
190.356270	14.777606	75.634804
190.062591	-25.343269	75.639809
189.231538	22.401428	75.644814
187.989389	2.336628	75.649818
188.031232	4.443009	75.654823
187.585438	10.462095	75.659828
186.384362	-25.111479	75.664833
185.876352	11.275508	75.669838
184.978367	-15.269904	75.674842
184.889934	2.339000	75.679847
184.095859	-18.185114	75.684852
183.552355	-1.743088	75.689857
182.562833	-19.839190	75.694862
181.902209	24.137999	75.699866
181.418136	-19.959378	75.704871
180.913839	19.432557	75.709876
180.175829	-18.411442	75.714881
179.248765	1.620780	75.719886
178.256748	-1.586080	75.724890
177.898559	-18.880858	75.729895
177.186000	16.568974	75.734900
176.729994	-20.870565	75.739905
176.124275	12.461830	75.744910
174.874498	-10.602523	75.749914
174.814818	13.832829	75.754919
174.187809	-11.499013	75.759924
173.429464	17.163372	75.764929
172.770912	-10.747943	75.769934
171.859506	2.840257	75.774938
171.585915	1.168274	75.779943
170.517752	-10.688213	75.784948
169.894070	-2.936170	75.789953
169.703486	2.340517	75.794958
168.896608	-7.244352	75.799962
167.933728	3.275574	75.804967
167.530505	-31.758150	75.809972
166.997948	0.148097	75.814977
165.967039	14.231577	75.819982
164.652215	-3.516218	75.824986
164.686352	-20.463552	75.829991
163.990986	16.073156	75.834996
163.404208	-1.323959	75.840001
163.793898	-23.706694	75.845006
162.405350	21.132396	75.850010
161.636433	11.848956	75.855015
160.518059	-11.045533	75.860020
159.791447	-13.145155	75.865025
159.372834	-17.447890	75.870030
158.695497	-29.074945	75.875034
158.648280	5.973907	75.880039
157.504027	-32.962695	75.885044
156.480115	6.264475	75.890049
156.658784	-2.365826	75.895054
155.711219	-22.286733	75.900058
155.252458	-25.946008	75.905063
154.138039	14.055665	75.910068
153.293700	-6.200250	75.915073
152.973760	-38.339473	75.920078
151.577516	14.645364	75.925082
151.524958	0.042454	75.930087
151.042942	-24.877252	75.935092
150.457804	-42.211499	75.940097
149.421129	-37.626207	75.945102
148.531467	13.292576	75.950106
148.559079	14.827244	75.955111
148.296376	-21.698547	75.960116
147.106403	2.634732	75.965121
146.401659	6.829664	75.970126
145.516681	-20.577183	75.975130
144.929700	-39.995761	75.980135
143.816124	-12.197688	75.985140
143.302384	23.280378	75.990145
142.701276	-7.890027	75.995150
142.709917	-29.213836	76.000154
141.627532	-3.189968	76.005159
140.835696	19.980779	76.010164
140.362109	4.465756	76.015169
139.581412	0.942960	76.020174
139.350076	-30.251661	76.025178
138.873285	-2.818437	76.030183
138.129442	-13.026744	76.035188
137.107406	-4.675044	76.040193
136.363556	-23.456802	76.045198
135.630573	22.384732	76.050202
134.969235	7.588739	76.055207
134.109205	-5.903022	76.060212
133.163381	-14.699355	76.065217
133.276361	-27.039009	76.070222
132.741934	25.102015	76.075226
131.886375	-7.426504	76.080231
131.274331	-10.889458	76.085236
130.444342	9.989854	76.090241
130.346606	-14.767215	76.095246
128.699633	11.852879	76.100250
128.480018	-8.814850	76.105255
127.601869	1.526004	76.110260
127.334062	-6.314049	76.115265
126.338671	-12.409177	76.120270
125.708364	3.239338	76.125274
125.249109	-19.164149	76.130279
124.489437	5.784891	76.135284
123.684381	-11.050714	76.140289
123.197747	-20.213555	76.145294
122.302768	10.768105	76.150298
122.315448	-14.216292	76.155303
121.265788	-9.274114	76.160308
120.598724	-37.392137	76.165313
120.271832	7.462126	76.170318
118.766833	-19.927839	76.175322
118.219727	-3.767499	76.180327
117.821027	-14.701000	76.185332
117.243759	-19.164499	76.190337
116.773672	-4.229055	76.195342
115.745712	-8.761035	76.200346
115.211978	-17.755524	76.205351
114.993729	6.217831	76.210356
114.000910	-11.002549	76.215361
113.079876	-9.234623	76.220366
112.307863	0.125841	76.225370
111.534627	-8.306941	76.230375
111.621355	-9.147013	76.235380
110.658071	-4.751586	76.240385
109.801311	-24.182343	76.245390
108.930816	-12.967551	76.250394
109.005499	-6.613585	76.255399
108.056064	0.163869	76.260404
107.287821	-25.621608	76.265409
106.816510	-3.864422	76.270414
105.931774	-21.400048	76.275418
105.297840	-20.988281	76.280423
104.272035	3.285716	76.285428
103.863633	-35.869085	76.290433
103.746758	1.568763	76.295438
102.280007	-19.615979	76.300442
101.724797	2.783767	76.305447
101.239754	-23.401665	76.310452
101.129877	-18.670836	76.315457
100.494202	-4.532115	76.320462
99.352359	-20.542902	76.325466
98.439598	2.005316	76.330471
98.277751	-25.051623	76.335476
97.300035	-1.097521	76.340481
97.070227	-25.887114	76.345486
96.027737	-4.483527	76.350490
96.128328	-14.063261	76.355495
94.581376	-24.129286	76.360500
94.096840	-14.199689	76.365505
93.645419	-20.053550	76.370510
92.586139	7.180850	76.375514
92.191971	-39.972531	76.380519
91.426254	-5.580248	76.385524
90.921816	-13.373096	76.390529
90.105328	-12.569534	76.395534
88.976802	-5.637369	76.400538
88.763792	-14.101128	76.405543
88.271811	-22.331173	76.410548
87.646752	-0.852226	76.415553
86.762572	-22.714868	76.420558
85.692448	3.840048	76.425562
86.028218	-24.373244	76.430567
85.129803	8.505936	76.435572
84.278672	-19.196415	76.440577
83.648405	16.342781	76.445582
82.524962	-3.990009	76.450586
82.510195	-15.631241	76.455591
81.500048	-22.182860	76.460596
80.857138	0.603009	76.465601
80.693682	-25.206359	76.470606
79.126281	14.407104	76.475610
78.659600	-28.417257	76.480615
78.108678	1.142372	76.485620
77.973287	-25.434677	76.490625
77.082195	-9.708317	76.495630
76.071592	-9.367356	76.500634
75.628084	-22.203286	76.505639
75.419944	2.509572	76.510644
74.268795	-26.081578	76.515649
73.348645	-1.900124	76.520654
72.765607	-4.689632	76.525658
72.594793	-25.473906	76.530663
71.360396	-15.073085	76.535668
70.685598	-0.379366	76.540673
70.325541	-13.157651	76.545678
69.633736	-11.981325	76.550682
69.345990	-15.212138	76.555687
68.564319	-21.527388	76.560692
67.837636	-11.693205	76.565697
67.496506	-17.528381	76.570702
65.944919	-15.145824	76.575706
65.561493	-14.597386	76.580711
65.009671	-14.290162	76.585716
64.750075	-11.044521	76.590721
63.771804	-15.343137	76.595726
62.730518	-11.329474	76.600730
62.056379	-20.897610	76.605735
61.883703	-11.825100	76.610740
60.963448	-8.228109	76.615745
60.375743	-24.735647	76.620750
59.682712	-13.027201	76.625754
59.346886	-10.903173	76.630759
58.263565	-19.269131	76.635764
57.331343	-19.601371	76.640769
56.961742	-3.127154	76.645774
56.154326	-13.293750	76.650778
56.454601	-23.439880	76.655783
55.281213	-5.799901	76.660788
54.597161	-0.289983	76.665793
54.348762	-25.027713	76.670798
53.313162	14.683863	76.675802
51.944057	-20.992107	76.680807
52.145935	-36.758270	76.685812
50.918266	5.481672	76.690817
50.163864	-21.111768	76.695822
49.698005	-35.550944	76.700826
49.211086	-0.890896	76.705831
48.844774	-27.424796	76.710836
48.039402	7.268712	76.715841
47.482605	-21.604861	76.720846
46.344287	-5.419615	76.725850
46.366587	-6.918008	76.730855
44.986637	-18.683693	76.735860
44.485768	1.536032	76.740865
44.195225	-17.013644	76.745870
42.873816	6.547459	76.750874
42.436812	-29.474244	76.755879
41.511733	18.468324	76.760884
40.741822	-2.956828	76.765889
41.082463	-33.804247	76.770894
40.439066	-9.985467	76.775898
39.664727	-12.416467	76.780903
38.784235	-18.496760	76.785908
37.741613	-15.840562	76.790913
37.209099	-10.238123	76.795918
36.455812	-15.075630	76.800922
35.944962	-25.103435	76.805927
35.480589	-7.343152	76.810932
34.756679	-18.620555	76.815937
33.965853	-23.024740	76.820942
33.085814	-8.865966	76.825946
33.077496	-27.809123	76.830951
31.747773	-20.942621	76.835956
31.228047	-19.949839	76.840961
30.905147	-22.571097	76.845966
30.245059	-11.441880	76.850970
29.393173	-31.308575	76.855975
28.242079	3.242952	76.860980
27.862236	-21.107977	76.865985
27.760704	-25.248375	76.870990
26.742458	0.754250	76.875994
26.128853	-33.963576	76.880999
25.425979	-9.523485	76.886004
24.831626	-7.120113	76.891009
24.090325	-32.461992	76.896014
22.879800	-5.988767	76.901018
22.819479	-13.645856	76.906023
22.351871	-8.099495	76.911028
21.497249	-12.695343	76.916033
20.713043	-20.870877	76.921038
19.980409	0.833378	76.926042
20.088740	-19.328393	76.931047
18.666858	-10.096067	76.936052
17.736435	-1.678519	76.941057
17.778635	-13.697817	76.946062
17.105846	-21.272986	76.951066
16.398348	0.425682	76.956071
15.687996	-16.503809	76.961076
14.740840	-6.021046	76.966081
14.125721	-6.446422	76.971086
13.081994	-0.590561	76.976090
12.857666	-6.441206	76.981095
12.224534	-9.016137	76.986100
11.478204	-0.855018	76.991105
10.728443	-5.898074	76.996110
9.622472	-6.331888	77.001114
9.464920	4.472777	77.006119
9.202816	-16.542922	77.011124
8.484544	5.587959	77.016129
7.814840	-27.452591	77.021134
6.830796	-0.266462	77.026139
6.719808	-9.689451	77.031143
5.580652	-22.382867	77.036148
4.939866	-5.942669	77.041153
4.589457	-3.603431	77.046158