Mon Mar 08 18:42:02 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.452952	80.952122	0.000000
-1.497640	97.412391	0.005005
-2.478834	52.557075	0.010010
-3.757336	10.179269	0.015014
-8.241073	15.393227	0.020019
-12.842857	-17.534106	0.025024
-18.303776	25.467608	0.030029
-22.905364	-3.534942	0.035034
-26.402818	-15.391708	0.040038
-30.670654	24.660218	0.045043
-34.297682	-11.437527	0.050048
-37.561795	18.742397	0.055053
-41.451302	-12.021502	0.060058
-44.973736	-6.132967	0.065062
-49.185273	14.561874	0.070067
-52.691452	-11.225063	0.075072
-56.161639	-23.920285	0.080077
-59.992164	-21.744981	0.085082
-63.545288	6.864763	0.090086
-67.967765	15.612271	0.095091
-72.166166	-13.142247	0.100096
-75.547828	-35.279605	0.105101
-79.205962	9.553887	0.110106
-82.790285	18.759041	0.115110
-86.578352	-9.091142	0.120115
-90.182838	-5.825968	0.125120
-94.069613	31.577637	0.130125
-98.361913	11.460412	0.135130
-101.061403	-33.842626	0.140134
-105.223667	27.770323	0.145139
-109.304685	21.670859	0.150144
-112.927684	-14.738014	0.155149
-116.851040	23.931348	0.160154
-120.378657	-18.101628	0.165158
-124.285201	16.279134	0.170163
-127.980988	13.541618	0.175168
-131.611587	-14.235827	0.180173
-135.659297	0.346304	0.185178
-139.036124	13.857953	0.190182
-143.135979	-7.453585	0.195187
-146.855087	-24.311283	0.200192
-150.599101	16.346288	0.205197
-154.273757	25.635339	0.210202
-157.693075	-12.206208	0.215206
-161.591610	-5.429650	0.220211
-165.415602	17.296029	0.225216
-169.680231	-0.709300	0.230221
-173.288478	-25.027426	0.235226
-177.077555	9.057112	0.240230
-181.593313	0.739125	0.245235
-184.795948	-18.663983	0.250240
-188.413001	15.125068	0.255245
-191.866833	-4.591184	0.260250
-195.449287	-2.092573	0.265254
-199.856240	4.635874	0.270259
-202.826284	-15.993280	0.275264
-207.356430	-2.374785	0.280269
-210.885174	-24.234592	0.285274
-214.279234	12.223209	0.290278
-218.655622	-10.460072	0.295283
-222.275862	-5.952781	0.300288
-225.606239	16.560171	0.305293
-229.585117	-0.096695	0.310298
-232.670141	-30.485545	0.315302
-237.019910	16.491072	0.320307
-241.019680	27.122005	0.325312
-244.832960	10.205351	0.330317
-248.232435	-22.198996	0.335322
-252.067512	-21.690982	0.340326
-256.136581	21.144200	0.345331
-259.818782	25.571562	0.350336
-263.772052	6.013967	0.355341
-267.355348	-0.669241	0.360346
-270.370462	-31.491784	0.365350
-274.751180	7.944536	0.370355
-278.432955	8.857031	0.375360
-281.901156	-25.847957	0.380365
-286.460462	-23.866622	0.385370
-289.569945	10.595256	0.390374
-293.868393	28.005564	0.395379
-297.427191	-4.729676	0.400384
-301.168379	-27.928858	0.405389
-305.166944	16.948184	0.410394
-308.581595	11.185810	0.415398
-312.240375	-11.482516	0.420403
-315.820732	-9.556465	0.425408
-319.718586	-1.494632	0.430413
-323.953201	-0.919574	0.435418
-327.527446	20.399323	0.440422
-331.244347	-7.660447	0.445427
-334.785058	20.696934	0.450432
-338.595232	-26.095186	0.455437
-342.536442	15.648988	0.460442
-346.193226	6.112476	0.465446
-349.843387	-26.764141	0.470451
-353.404507	-34.038905	0.475456
-357.002871	-4.316248	0.480461
-361.237605	21.553296	0.485466
-365.373328	4.101746	0.490470
-368.905998	-5.235352	0.495475
-372.269633	-25.757256	0.500480
-376.399254	6.833409	0.505485
-380.386218	13.170294	0.510490
-383.728223	-22.533892	0.515494
-387.715206	-26.837626	0.520499
-391.510474	26.108971	0.525504
-395.089363	32.823835	0.530509
-399.198954	25.157311	0.535514
-402.716610	-10.411601	0.540518
-406.386777	2.929601	0.545523
-410.024746	30.045859	0.550528
-413.704596	31.456540	0.555533
-417.746784	-4.022304	0.560538
-421.318343	0.035986	0.565542
-425.635209	37.325756	0.570547
-429.649994	3.717430	0.575552
-432.516913	-23.195849	0.580557
-436.336751	32.268244	0.585562
-440.322202	4.879124	0.590566
-444.591300	7.454625	0.595571
-447.445270	-21.444390	0.600576
-451.283370	18.323425	0.605581
-455.687046	23.544330	0.610586
-458.971663	-6.832831	0.615590
-462.572691	14.261859	0.620595
-466.424376	27.597460	0.625600
-470.215783	-7.419871	0.630605
-474.267498	4.828096	0.635610
-478.024440	12.110786	0.640614
-481.554096	-21.541729	0.645619
-485.297557	9.661290	0.650624
-489.305805	43.590481	0.655629
-493.432890	31.554282	0.660634
-496.870741	9.845969	0.665638
-500.303024	4.296421	0.670643
-504.502160	18.829201	0.675648
-508.275129	8.947252	0.680653
-511.419609	-11.634674	0.685658
-514.959036	2.710754	0.690662
-519.379747	28.503018	0.695667
-523.303541	2.096065	0.700672
-526.314105	-15.456004	0.705677
-530.502834	-11.731049	0.710682
-534.172315	26.888812	0.715686
-538.048773	45.572463	0.720691
-541.788505	24.727654	0.725696
-545.751057	28.758698	0.730701
-549.634922	28.641081	0.735706
-553.310234	9.703486	0.740710
-557.255681	6.692727	0.745715
-560.187660	-10.163842	0.750720
-563.989118	-20.818513	0.755725
-568.242873	25.867274	0.760730
-571.688767	29.188247	0.765734
-575.683007	22.761951	0.770739
-579.315362	3.420180	0.775744
-583.265791	-26.255900	0.780749
-587.067398	-17.311808	0.785754
-590.471609	-27.501637	0.790758
-594.866812	-11.969236	0.795763
-598.513952	29.799265	0.800768
-602.212104	3.629214	0.805773
-605.753039	-7.696176	0.810778
-609.379304	27.345294	0.815782
-613.488742	5.463785	0.820787
-617.065412	-0.103519	0.825792
-620.829632	27.012660	0.830797
-625.301594	13.852328	0.835802
-628.070152	-10.042525	0.840806
-631.937031	-1.554678	0.845811
-635.228637	-25.417972	0.850816
-639.423391	5.072049	0.855821
-643.622427	43.480226	0.860826
-647.470188	32.265386	0.865830
-651.089295	20.392750	0.870835
-654.865888	7.936625	0.875840
-658.387621	7.602070	0.880845
-662.582568	6.566151	0.885850
-665.443874	-31.863416	0.890854
-669.685335	19.617293	0.895859
-673.333082	37.449351	0.900864
-677.305592	15.151863	0.905869
-681.360413	12.756415	0.910874
-685.047516	-0.842975	0.915878
-688.455337	-17.449871	0.920883
-692.134083	-6.771788	0.925888
-695.599067	18.352401	0.930893
-699.772175	31.261918	0.935898
-703.344657	27.919013	0.940902
-707.296092	31.272072	0.945907
-711.045910	18.630418	0.950912
-715.118836	0.139829	0.955917
-719.246262	42.455140	0.960922
-722.389224	37.269666	0.965926
-725.977599	40.667239	0.970931
-729.887479	30.947869	0.975936
-733.542185	14.342615	0.980941
-737.905117	7.992871	0.985946
-741.575685	16.995118	0.990950
-745.098799	33.388184	0.995955
-748.508631	-21.647777	1.000960
-752.394419	-15.559849	1.005965
-756.344572	28.439599	1.010970
-759.852426	-8.172514	1.015974
-763.525302	-20.332783	1.020979
-767.398926	-18.554727	1.025984
-771.216880	-17.979236	1.030989
-775.500145	8.221911	1.035994
-778.722550	8.405789	1.040998
-782.762673	17.944942	1.046003
-786.193813	11.391185	1.051008
-789.718145	14.430128	1.056013
-794.187319	12.192556	1.061018
-797.517445	0.658748	1.066022
-801.148633	-5.913465	1.071027
-804.408346	-16.515546	1.076032
-808.750318	22.273587	1.081037
-812.927863	21.940006	1.086042
-816.630385	-16.135721	1.091046
-820.553211	-14.176262	1.096051
-823.973857	-26.531268	1.101056
-827.844425	19.768753	1.106061
-831.662378	25.551108	1.111066
-835.691873	8.138674	1.116070
-838.957334	-0.934479	1.121075
-842.266357	-28.012991	1.126080
-846.269630	9.252400	1.131085
-850.721342	38.465619	1.136090
-854.278403	15.789846	1.141094
-858.309667	13.130762	1.146099
-861.545521	7.638663	1.151104
-865.098481	-12.249829	1.156109
-868.828315	-17.574640	1.161114
-872.499299	-26.560826	1.166118
-876.585284	31.415584	1.171123
-880.240822	35.938956	1.176128
-883.797739	17.973271	1.181133
-888.145118	-7.717151	1.186138
-891.544531	21.242726	1.191142
-895.544242	6.716016	1.196147
-899.283883	-0.663396	1.201152
-903.062676	19.758587	1.206157
-907.260905	1.881296	1.211162
-909.960272	-28.471915	1.216166
-913.907142	16.763406	1.221171
-917.811894	33.709689	1.226176
-921.815152	14.859858	1.231181
-925.450991	-6.032356	1.236186
-929.344585	10.393351	1.241190
-933.138089	5.730055	1.246195
-936.970172	10.955046	1.251200
-940.631304	15.651275	1.256205
-944.347291	1.274829	1.261210
-948.348874	25.037577	1.266214
-952.216036	3.706173	1.271219
-955.205830	12.830100	1.276224
-959.511347	12.753770	1.281229
-963.420975	7.560348	1.286234
-966.174542	-19.228339	1.291238
-970.520500	35.232393	1.296243
-974.541114	1.386454	1.301248
-978.223695	11.009087	1.306253
-982.532124	15.324789	1.311258
-985.505118	-2.347737	1.316262
-989.560352	18.213177	1.321267
-992.902645	-21.834078	1.326272
-996.805572	14.335335	1.331277
-1000.652534	-13.404339	1.336282
-1004.213348	13.826430	1.341286
-1008.533179	-5.847734	1.346291
-1012.113831	9.157771	1.351296
-1016.163744	7.127955	1.356301
-1019.371543	-5.470517	1.361306
-1023.347471	20.787530	1.366310
-1026.926781	-0.911435	1.371315
-1030.823347	8.956792	1.376320
-1034.451113	3.779915	1.381325
-1039.062583	9.973322	1.386330
-1042.014442	-19.413721	1.391334
-1046.091103	24.207348	1.396339
-1049.631440	-10.506793	1.401344
-1052.844148	-4.622217	1.406349
-1057.069515	33.554176	1.411354
-1060.780453	-1.478011	1.416358
-1064.761580	-4.304010	1.421363
-1068.839959	15.041819	1.426368
-1072.107204	-19.845235	1.431373
-1075.957709	27.041619	1.436378
-1079.711254	-2.214023	1.441382
-1083.605533	-11.574133	1.446387
-1087.451777	23.304376	1.451392
-1091.343634	-1.528140	1.456397
-1094.660251	-16.687224	1.461402
-1098.355687	23.854855	1.466406
-1102.299025	8.181030	1.471411
-1105.695974	-8.936254	1.476416
-1110.017378	16.831580	1.481421
-1113.600300	-11.426319	1.486426
-1117.392313	1.080719	1.491430
-1121.200322	2.716403	1.496435
-1125.171051	7.744688	1.501440
-1128.131700	-28.329771	1.506445
-1132.330011	20.145450	1.511450
-1135.988359	-1.124390	1.516454
-1139.667922	-9.550566	1.521459
-1144.069453	12.891954	1.526464
-1147.392968	-17.657526	1.531469
-1151.354765	33.492098	1.536474
-1154.851368	-10.618965	1.541478
-1158.809746	17.460868	1.546483
-1162.423634	0.558132	1.551488
-1166.273977	1.532079	1.556493
-1169.947063	-21.427265	1.561498
-1173.781642	16.823913	1.566502
-1177.912860	-9.717271	1.571507
-1181.546548	10.306582	1.576512
-1184.887924	-2.596677	1.581517
-1188.666563	14.824937	1.586522
-1192.197044	5.411536	1.591526
-1196.064874	-7.062145	1.596531
-1200.340995	-7.467563	1.601536
-1203.797961	8.414061	1.606541
-1207.959553	-3.410247	1.611546
-1211.211299	-7.570012	1.616550
-1215.269282	10.009862	1.621555
-1218.948236	-4.282142	1.626560
-1222.339946	3.473053	1.631565
-1226.614718	13.337451	1.636570
-1230.339765	-5.972558	1.641574
-1234.242756	-2.262137	1.646579
-1237.715536	-4.749735	1.651584
-1241.192848	-1.438553	1.656589
-1245.220800	0.081149	1.661594
-1248.885530	-8.886499	1.666598
-1252.542881	18.531905	1.671603
-1256.443348	-1.183625	1.676608
-1260.135340	-10.876968	1.681613
-1264.147188	4.850689	1.686618
-1267.278791	-7.754866	1.691622
-1271.812937	-1.138183	1.696627
-1275.810837	11.040949	1.701632
-1279.302688	-3.310851	1.706637
-1282.815155	8.863143	1.711642
-1286.327810	11.751148	1.716646
-1290.692608	-2.662772	1.721651
-1293.834579	-14.333132	1.726656
-1297.757288	28.363253	1.731661
-1302.076995	8.202415	1.736666
-1305.058496	10.174448	1.741670
-1309.170954	-5.323686	1.746675
-1313.028175	6.910253	1.751680
-1316.462500	-4.326966	1.756685
-1320.849256	5.214916	1.761690
-1324.016648	7.719736	1.766694
-1328.202828	-2.007936	1.771699
-1331.727543	27.183801	1.776704
-1335.385182	-14.140060	1.781709
-1339.307392	-4.219949	1.786714
-1343.199165	15.638869	1.791718
-1346.976540	-12.555933	1.796723
-1350.741064	22.535315	1.801728
-1353.639784	-12.914824	1.806733
-1358.040199	20.538955	1.811738
-1361.498441	-7.199167	1.816742
-1365.491952	-5.774652	1.821747
-1369.589656	14.076167	1.826752
-1373.161910	7.801354	1.831757
-1376.859051	17.281841	1.836762
-1380.546079	-6.606821	1.841766
-1384.214982	17.486466	1.846771
-1388.122200	3.401589	1.851776
-1391.789096	-5.556012	1.856781
-1396.021887	26.059217	1.861786
-1399.347588	10.353304	1.866790
-1403.382432	-1.424690	1.871795
-1406.976003	15.163424	1.876800
-1410.379906	-9.055910	1.881805
-1414.771602	16.674774	1.886810
-1418.316797	7.806529	1.891814
-1421.838436	9.523005	1.896819
-1425.698393	9.391978	1.901824
-1429.764402	14.592130	1.906829
-1433.725760	4.639443	1.911834
-1437.006537	0.088864	1.916838
-1440.622335	15.434880	1.921843
-1444.340068	8.216870	1.926848
-1448.165636	-12.609327	1.931853
-1452.162292	6.340826	1.936858
-1455.844869	4.629841	1.941862
-1459.353560	2.920982	1.946867
-1463.158972	8.081043	1.951872
-1466.973972	-7.238916	1.956877
-1471.197337	16.427633	1.961882
-1474.619607	-6.367919	1.966886
-1478.820025	-7.365217	1.971891
-1482.502173	19.390450	1.976896
-1486.049908	-9.347021	1.981901
-1489.605042	7.249235	1.986906
-1493.003198	-8.843843	1.991910
-1497.054352	-4.576294	1.996915
-1501.161906	9.893474	2.006912
-1502.438491	3.967244	2.016909
-1499.558235	-0.628916	2.026906
-1496.773384	5.829575	2.036902
-1494.874967	12.164761	2.046899
-1493.022604	6.945344	2.056896
-1490.770651	3.626046	2.066893
-1488.834029	14.161199	2.076890
-1486.922420	14.054116	2.086886
-1485.125968	5.062291	2.096883
-1483.331919	7.037602	2.106880
-1481.420771	8.975220	2.116877
-1479.617472	7.949222	2.126874
-1477.786605	10.139684	2.136870
-1475.539465	-0.038967	2.146867
-1473.957836	13.017634	2.156864
-1471.762516	1.284212	2.166861
-1469.795922	-7.625895	2.176858
-1468.460450	12.848123	2.186854
-1466.229829	26.741834	2.196851
-1464.386316	-3.287916	2.206848
-1462.037969	10.931126	2.216845
-1460.524011	13.800728	2.226842
-1459.173583	8.124886	2.236838
-1456.946053	19.668175	2.246835
-1455.068412	9.820257	2.256832
-1452.950433	11.293756	2.266829
-1450.994340	12.674761	2.276826
-1449.341458	9.380366	2.286822
-1447.433143	-3.027043	2.296819
-1445.207509	9.283879	2.306816
-1443.772817	-2.304058	2.316813
-1441.817165	32.774631	2.326810
-1439.950575	35.159924	2.336806
-1438.054098	16.606313	2.346803
-1435.762395	-1.664777	2.356800
-1434.058477	12.805883	2.366797
-1432.690804	10.605522	2.376794
-1430.494883	7.582603	2.386790
-1428.426935	24.742217	2.396787
-1426.549041	16.384720	2.406784
-1424.804538	1.155285	2.416781
-1422.860623	21.667728	2.426778
-1420.863503	4.149554	2.436774
-1419.120914	-1.982180	2.446771
-1417.252794	4.684746	2.456768
-1415.515305	13.649305	2.466765
-1413.666243	7.953659	2.476762
-1411.449680	-12.462092	2.486758
-1409.755425	8.657124	2.496755
-1408.141807	-2.370524	2.506752
-1405.726350	-3.113955	2.516749
-1404.454882	16.951969	2.526746
-1402.124252	7.495760	2.536742
-1400.106778	-5.105921	2.546739
-1398.572821	8.732012	2.556736
-1396.626305	2.842369	2.566733
-1394.651353	4.967203	2.576730
-1392.973716	7.858014	2.586726
-1391.057271	8.765444	2.596723
-1389.289041	-10.050190	2.606720
-1387.328148	13.555704	2.616717
-1385.323638	8.806194	2.626714
-1383.544177	9.568199	2.636710
-1381.445201	14.958802	2.646707
-1379.825917	-1.662061	2.656704
-1377.722883	28.069193	2.666701
-1375.895484	19.582452	2.676698
-1374.119197	13.202204	2.686694
-1372.095791	6.896083	2.696691
-1370.332635	8.336460	2.706688
-1368.603092	3.602560	2.716685
-1366.595479	11.635023	2.726682
-1364.707572	6.553688	2.736678
-1362.471465	7.706801	2.746675
-1360.660277	15.612828	2.756672
-1359.291195	14.945356	2.766669
-1357.342695	3.341528	2.776666
-1355.450029	14.368554	2.786662
-1353.213166	12.198053	2.796659
-1351.383010	8.595891	2.806656
-1349.692771	13.958794	2.816653
-1347.840591	2.602483	2.826650
-1345.816864	18.349862	2.836646
-1343.966362	3.544008	2.846643
-1342.141774	15.881346	2.856640
-1340.265650	8.547301	2.866637
-1338.686852	11.521865	2.876634
-1336.349690	6.212340	2.886630
-1334.560044	13.288197	2.896627
-1332.672169	-5.593927	2.906624
-1330.860095	39.336301	2.916621
-1328.980051	10.513306	2.926618
-1327.241948	18.009504	2.936614
-1325.279848	12.106367	2.946611
-1323.349822	9.844484	2.956608
-1321.314660	25.907418	2.966605
-1320.025977	35.820171	2.976602
-1317.776417	11.736210	2.986598
-1315.760572	4.905583	2.996595
-1314.032144	4.234309	3.006592
-1312.094392	19.725499	3.016589
-1310.281859	10.906469	3.026586
-1308.421355	13.374943	3.036582
-1306.270727	9.348915	3.046579
-1304.463995	14.314284	3.056576
-1302.661003	7.955076	3.066573
-1301.046764	17.567847	3.076570
-1298.941843	6.351108	3.086566
-1297.115401	10.811249	3.096563
-1295.267996	7.880543	3.106560
-1293.407395	11.760516	3.116557
-1291.674701	20.915416	3.126554
-1289.517161	1.993311	3.136550
-1287.529126	20.962607	3.146547
-1285.739615	12.287796	3.156544
-1283.748790	12.523448	3.166541
-1282.208220	6.383083	3.176538
-1280.128766	3.821023	3.186534
-1278.466301	5.296530	3.196531
-1276.513506	13.445216	3.206528
-1274.448507	17.112507	3.216525
-1272.584537	10.280955	3.226522
-1270.761842	10.058813	3.236518
-1269.086229	17.356649	3.246515
-1267.165136	15.358332	3.256512
-1265.253415	11.785811	3.266509
-1263.366461	12.928581	3.276506
-1261.418107	8.699710	3.286502
-1259.566110	6.920867	3.296499
-1257.441497	11.960137	3.306496
-1255.651930	5.074193	3.316493
-1253.830005	11.263947	3.326490
-1252.337443	16.361734	3.336486
-1250.100904	7.776462	3.346483
-1248.138920	3.900666	3.356480
-1246.670562	17.783963	3.366477
-1244.632077	14.914293	3.376474
-1242.539499	3.159605	3.386470
-1241.058386	24.594151	3.396467
-1238.824738	7.309810	3.406464
-1236.934207	4.861696	3.416461
-1235.043378	10.525732	3.426458
-1233.336493	18.645919	3.436454
-1231.399693	16.814055	3.446451
-1229.380267	13.990077	3.456448
-1227.455954	-1.691147	3.466445
-1225.487512	8.318138	3.476442
-1224.292104	18.662688	3.486438
-1222.364051	2.301953	3.496435
-1220.333042	10.147665	3.506432
-1218.071394	5.780285	3.516429
-1216.341710	4.058938	3.526426
-1214.561531	20.816426	3.536422
-1212.357611	12.773217	3.546419
-1210.835227	5.096413	3.556416
-1209.014143	11.128454	3.566413
-1206.952474	3.286426	3.576410
-1205.128971	19.130722	3.586406
-1203.298198	10.608831	3.596403
-1201.147076	13.471399	3.606400
-1199.329363	1.692830	3.616397
-1197.867233	8.849622	3.626394
-1196.064987	14.493131	3.636390
-1193.830465	1.976863	3.646387
-1192.186484	1.559176	3.656384
-1190.179711	-4.259423	3.666381
-1188.157828	2.386261	3.676378
-1186.339746	9.817674	3.686374
-1184.440371	11.010625	3.696371
-1182.552101	8.373451	3.706368
-1180.614705	4.405332	3.716365
-1179.003224	24.271789	3.726362
-1176.833159	13.684158	3.736358
-1175.092761	-2.182332	3.746355
-1173.287723	11.907666	3.756352
-1171.553472	10.300878	3.766349
-1169.470192	21.802827	3.776346
-1167.575954	-0.492150	3.786342
-1165.657932	11.852505	3.796339
-1163.569286	4.413542	3.806336
-1161.973404	-1.678758	3.816333
-1160.298831	0.906418	3.826330
-1158.106083	18.554747	3.836326
-1156.307016	10.404258	3.846323
-1154.438997	7.432469	3.856320
-1152.674288	-2.169807	3.866317
-1150.594943	12.122635	3.876314
-1148.554641	14.980877	3.886310
-1147.150526	15.945208	3.896307
-1145.093558	10.690159	3.906304
-1143.210888	6.481363	3.916301
-1141.362113	3.732125	3.926298
-1139.425525	10.486236	3.936294
-1137.473316	13.109120	3.946291
-1135.747593	8.126530	3.956288
-1133.785309	4.097627	3.966285
-1131.984233	14.141672	3.976282
-1130.269612	26.095775	3.986278
-1128.033771	9.714278	3.996275
-1125.983526	12.686207	4.006272
-1124.534935	20.959901	4.016269
-1122.775679	12.951584	4.026266
-1120.836481	10.101059	4.036262
-1118.843823	16.446769	4.046259
-1116.672069	13.413792	4.056256
-1115.359850	0.655139	4.066253
-1112.860030	5.029825	4.076250
-1111.151892	17.460212	4.086246
-1109.639955	4.336471	4.096243
-1107.675077	9.183553	4.106240
-1105.367718	17.858288	4.116237
-1103.785635	2.124519	4.126234
-1101.730337	13.886783	4.136230
-1100.056320	19.762453	4.146227
-1098.053839	0.764241	4.156224
-1096.317960	14.118573	4.166221
-1094.460209	11.007953	4.176218
-1092.476551	13.354281	4.186214
-1090.798512	9.669281	4.196211
-1088.749977	3.978284	4.206208
-1087.072729	-3.306395	4.216205
-1084.980202	9.741438	4.226202
-1083.240242	20.845252	4.236198
-1081.293056	-4.143792	4.246195
-1079.448394	15.353887	4.256192
-1077.220723	16.382319	4.266189
-1075.673937	15.667644	4.276186
-1073.756449	7.821939	4.286182
-1072.226497	30.241937	4.296179
-1069.807644	0.170864	4.306176
-1068.120010	15.315478	4.316173
-1066.298709	3.473265	4.326170
-1064.339638	18.157652	4.336166
-1062.671148	24.638944	4.346163
-1060.631831	14.111790	4.356160
-1058.779705	8.141191	4.366157
-1056.570086	9.046220	4.376154
-1055.151334	22.315533	4.386150
-1053.227157	10.906847	4.396147
-1051.069719	5.698963	4.406144
-1049.274909	8.771810	4.416141
-1047.543861	19.510783	4.426138
-1045.814642	7.457529	4.436134
-1043.728084	17.193906	4.446131
-1041.852079	24.182000	4.456128
-1040.188636	13.167107	4.466125
-1038.152561	14.202535	4.476122
-1035.961497	18.175133	4.486118
-1034.417555	14.011115	4.496115
-1032.349785	11.053261	4.506112
-1030.583988	-4.899308	4.516109
-1028.535777	7.243085	4.526106
-1027.061534	21.043516	4.536102
-1024.814037	-7.768589	4.546099
-1023.285822	36.487458	4.556096
-1021.326307	6.415656	4.566093
-1019.497098	23.857036	4.576090
-1017.593252	14.819926	4.586086
-1015.420660	10.748011	4.596083
-1013.913588	31.130247	4.606080
-1011.474006	-10.362456	4.616077
-1010.083625	34.480875	4.626074
-1008.239476	18.563129	4.636070
-1006.693607	18.094950	4.646067
-1003.989172	-17.205132	4.656064
-1002.387050	-24.785612	4.666061
-1000.291610	3.081057	4.676058
-998.715097	47.787314	4.686054
-997.243340	15.892540	4.696051
-994.754334	1.220058	4.706048
-993.102609	46.708461	4.716045
-991.041469	42.637014	4.726042
-989.347388	9.391506	4.736038
-987.383118	-16.111750	4.746035
-985.776093	28.959039	4.756032
-983.994121	1.684992	4.766029
-981.436050	18.141480	4.776026
-980.493900	19.407139	4.786022
-977.982021	16.926185	4.796019
-976.048725	42.280066	4.806016
-974.225123	2.144203	4.816013
-972.070013	-20.648639	4.826010
-970.434830	-9.400110	4.836006
-969.071939	19.254778	4.846003
-967.021957	41.223862	4.856000
-964.877328	32.059862	4.865997
-963.114258	28.992896	4.875994
-961.296691	17.798674	4.885990
-959.080489	-2.076734	4.895987
-957.132307	-7.371068	4.905984
-955.593847	36.057670	4.915981
-954.288234	17.559353	4.925978
-951.589410	-0.219115	4.935974
-950.034715	6.517281	4.945971
-947.568012	-9.545722	4.955968
-946.120638	-6.038318	4.965965
-944.701794	13.881243	4.975962
-942.554460	17.054122	4.985958
-940.135833	-16.223473	4.995955
-938.600192	28.137242	5.005952
-936.873751	34.765680	5.015949
-934.833398	40.407663	5.025946
-932.935488	41.089505	5.035942
-931.219108	39.897830	5.045939
-929.351275	-4.054890	5.055936
-927.878919	14.384626	5.065933
-925.247826	15.896574	5.075930
-923.744016	20.917008	5.085926
-921.732233	32.345390	5.095923
-919.871888	37.774598	5.105920
-917.821246	41.668721	5.115917
-916.175056	25.114810	5.125914
-914.700898	17.876908	5.135910
-912.772935	16.193550	5.145907
-910.174719	10.643752	5.155904
-908.457764	6.613198	5.165901
-906.385203	-22.420297	5.175898
-904.864628	-10.730256	5.185894
-903.182969	14.419161	5.195891
-901.267730	15.196146	5.205888
-898.844072	-7.424874	5.215885
-897.720933	12.235696	5.225882
-895.598536	19.018745	5.235878
-893.506818	40.608625	5.245875
-891.511305	-5.567017	5.255872
-890.153904	7.091719	5.265869
-888.541645	16.863023	5.275866
-885.907920	38.825714	5.285862
-884.001861	31.941917	5.295859
-882.584328	14.644625	5.305856
-880.510611	13.793740	5.315853
-878.507489	22.308948	5.325850
-876.748128	36.461810	5.335846
-874.860734	-7.846098	5.345843
-872.771824	-18.095241	5.355840
-870.971783	-22.734276	5.365837
-869.252523	-20.902834	5.375834
-867.261561	-20.548433	5.385830
-865.528430	12.834474	5.395827
-864.487895	17.723750	5.405824
-861.862422	18.775638	5.415821
-859.334485	28.522176	5.425818
-857.974789	10.154197	5.435814
-856.294185	-6.087797	5.445811
-854.397330	15.081681	5.455808
-851.984858	27.860747	5.465805
-850.460835	13.353683	5.475802
-848.648952	-1.418842	5.485798
-846.682222	34.925070	5.495795
-845.004624	36.895823	5.505792
-843.160324	12.196473	5.515789
-840.779521	9.795032	5.525786
-839.225120	1.968065	5.535782
-837.420532	29.016251	5.545779
-835.435483	14.675491	5.555776
-833.614779	13.726147	5.565773
-831.635499	8.215365	5.575770
-829.701904	14.580254	5.585766
-828.159505	21.479758	5.595763
-826.079541	29.619598	5.605760
-823.988931	11.910030	5.615757
-822.224821	5.374225	5.625754
-820.458022	37.542445	5.635750
-818.644266	4.707332	5.645747
-816.928804	26.808972	5.655744
-814.489572	6.241200	5.665741
-813.082853	23.600315	5.675738
-811.291894	8.368537	5.685734
-809.220104	34.199377	5.695731
-807.009487	-7.370303	5.705728
-805.715675	13.868766	5.715725
-803.763230	48.457765	5.725722
-801.650360	42.770913	5.735718
-800.092076	48.107984	5.745715
-797.838078	28.990785	5.755712
-795.795474	-14.209834	5.765709
-794.307870	14.049499	5.775706
-792.284772	10.260607	5.785702
-790.434837	9.938174	5.795699
-788.102242	-4.636493	5.805696
-786.756317	24.665460	5.815693
-785.114582	30.879683	5.825690
-782.877141	-3.060430	5.835686
-780.902590	24.229052	5.845683
-779.239807	-13.549009	5.855680
-777.545191	22.631614	5.865677
-775.408016	5.213053	5.875674
-773.537785	-2.274366	5.885670
-771.945748	24.525231	5.895667
-769.859731	18.792182	5.905664
-767.696680	1.457912	5.915661
-766.091433	13.241912	5.925658
-764.112544	20.921140	5.935654
-762.401850	17.171144	5.945651
-760.483511	4.279459	5.955648
-758.813294	-0.376650	5.965645
-756.507594	18.125621	5.975642
-754.173924	8.975804	5.985638
-753.035578	1.463257	5.995635
-751.035341	29.647056	6.005632
-749.227140	7.943915	6.015629
-747.076403	12.242170	6.025626
-745.447019	12.291316	6.035622
-743.719468	12.708441	6.045619
-741.387521	7.747660	6.055616
-739.896015	-4.357411	6.065613
-738.124607	20.149449	6.075610
-735.972146	-7.205778	6.085606
-733.993298	7.362089	6.095603
-732.487137	8.621403	6.105600
-730.361235	3.320944	6.115597
-728.334607	11.619384	6.125594
-726.613327	7.226701	6.135590
-724.785790	3.189655	6.145587
-722.998230	14.546684	6.155584
-721.206277	3.399349	6.165581
-719.113721	2.466651	6.175578
-717.158710	-3.889593	6.185574
-715.334172	5.378996	6.195571
-713.297358	-0.167725	6.205568
-711.662857	8.676520	6.215565
-709.715992	8.725484	6.225562
-707.837618	9.923762	6.235558
-706.397998	4.914550	6.245555
-704.088895	3.825692	6.255552
-702.132836	1.121220	6.265549
-700.287891	-0.641855	6.275546
-698.271937	-7.222548	6.285542
-696.724465	1.763498	6.295539
-694.780044	10.752440	6.305536
-692.972393	8.204313	6.315533
-691.023309	6.547756	6.325530
-688.823527	5.269547	6.335526
-687.097667	-4.027814	6.345523
-685.454105	18.495936	6.355520
-683.502613	4.809567	6.365517
-681.524250	6.689751	6.375514
-679.555578	3.738556	6.385510
-677.657755	10.377703	6.395507
-676.381597	6.599305	6.405504
-674.221165	0.530782	6.415501
-672.099792	1.126605	6.425498
-670.364953	1.796818	6.435494
-668.402433	-5.018461	6.445491
-666.615222	9.299053	6.455488
-664.767923	-2.584944	6.465485
-662.852052	12.503036	6.475482
-660.819691	-0.918351	6.485478
-658.843858	23.671193	6.495475
-657.418976	-0.961034	6.505472
-655.174070	1.193941	6.515469
-653.687418	7.753541	6.525466
-651.724548	4.465416	6.535462
-650.068339	-1.254122	6.545459
-647.996028	11.925285	6.555456
-645.727753	-5.177817	6.565453
-643.996036	3.215178	6.575450
-642.261797	-0.735852	6.585446
-640.100725	7.778021	6.595443
-638.634577	12.654673	6.605440
-636.524868	2.473424	6.615437
-634.566678	1.784886	6.625434
-632.791141	14.948567	6.635430
-630.801187	13.918658	6.645427
-629.131103	15.717090	6.655424
-627.455353	27.309960	6.665421
-625.569870	-6.100170	6.675418
-623.461588	11.892234	6.685414
-621.535063	10.563006	6.695411
-619.608747	7.148121	6.705408
-617.815947	29.944940	6.715405
-615.793142	8.850188	6.725402
-613.945667	5.152652	6.735398
-612.483796	10.852598	6.745395
-610.033894	14.302705	6.755392
-608.449192	1.543363	6.765389
-606.702329	33.020290	6.775386
-604.719540	0.649300	6.785382
-602.941455	11.810586	6.795379
-601.014399	13.817452	6.805376
-598.995403	11.128269	6.815373
-596.996567	-2.559283	6.825370
-595.242309	30.187462	6.835366
-593.463896	10.469068	6.845363
-591.317483	22.880426	6.855360
-589.893807	10.994663	6.865357
-587.813915	15.403856	6.875354
-585.846370	16.357473	6.885350
-584.216171	8.523277	6.895347
-581.917102	18.663518	6.905344
-580.115114	14.891169	6.915341
-578.555327	17.196707	6.925338
-576.390393	-5.412740	6.935334
-574.887911	32.396644	6.945331
-572.910479	33.358167	6.955328
-571.038943	19.842519	6.965325
-569.047824	0.154910	6.975322
-567.071147	24.420754	6.985318
-564.910205	19.165355	6.995315
-563.500259	35.870513	7.005312
-561.399899	20.933644	7.015309
-559.683947	9.681709	7.025306
-557.879352	26.909588	7.035302
-555.822745	1.309686	7.045299
-554.136704	7.346479	7.055296
-552.142931	10.956338	7.065293
-550.230155	3.946992	7.075290
-548.433365	1.386497	7.085286
-546.918988	6.995997	7.095283
-544.741889	-0.194501	7.105280
-542.832960	12.254827	7.115277
-540.925753	2.878064	7.125274
-538.888775	24.565480	7.135270
-537.056298	1.219707	7.145267
-535.188892	15.560854	7.155264
-533.364881	7.571003	7.165261
-531.324776	13.688631	7.175258
-529.633649	-3.402731	7.185254
-527.570275	31.197266	7.195251
-525.970506	-8.965831	7.205248
-523.954268	15.131102	7.215245
-522.458078	20.585642	7.225242
-520.363704	16.962420	7.235238
-518.260596	7.500702	7.245235
-516.500789	20.037033	7.255232
-514.617382	22.832486	7.265229
-512.646311	-3.101076	7.275226
-510.503057	0.251271	7.285222
-509.421866	6.733625	7.295219
-506.886197	0.761625	7.305216
-505.277920	4.406247	7.315213
-503.317332	26.401154	7.325210
-501.260148	13.492195	7.335206
-499.533310	10.226094	7.345203
-497.897123	1.107371	7.355200
-496.165086	16.968527	7.365197
-493.726116	-18.394563	7.375194
-492.271100	32.841339	7.385190
-490.018037	-7.228722	7.395187
-488.337545	35.468951	7.405184
-486.480523	34.795110	7.415181
-484.159697	23.217678	7.425178
-483.019229	25.934439	7.435174
-480.935630	-11.812854	7.445171
-479.232902	24.316289	7.455168
-476.873753	-5.945349	7.465165
-475.376947	23.902762	7.475162
-472.823970	3.748134	7.485158
-471.437177	-2.916645	7.495155
-469.843169	36.495014	7.505152
-467.725556	-4.709153	7.515149
-466.164663	27.392847	7.525146
-463.776742	22.477061	7.535142
-461.954120	16.906317	7.545139
-460.231457	19.545912	7.555136
-458.253110	8.338976	7.565133
-456.453326	35.040993	7.575130
-454.561348	-5.648737	7.585126
-452.685324	13.391422	7.595123
-450.608039	11.668798	7.605120
-448.676904	10.983153	7.615117
-447.305162	-6.775553	7.625114
-444.987749	29.531795	7.635110
-443.545426	34.720270	7.645107
-441.710324	0.877738	7.655104
-439.682639	20.684720	7.665101
-437.597810	-1.946587	7.675098
-435.774254	40.625694	7.685094
-434.119637	24.410142	7.695091
-431.662896	-1.806181	7.705088
-430.225702	-10.667305	7.715085
-428.268977	-6.787755	7.725082
-426.378310	23.726957	7.735078
-424.443699	-7.396819	7.745075
-422.792705	-5.653612	7.755072
-420.805763	19.990683	7.765069
-418.949465	21.895319	7.775066
-416.975822	16.328914	7.785062
-415.393222	3.014241	7.795059
-413.418204	8.922903	7.805056
-411.230549	16.127035	7.815053
-409.115241	17.843489	7.825050
-407.524025	9.996675	7.835046
-406.047582	35.187280	7.845043
-403.977989	10.734800	7.855040
-401.956885	2.216227	7.865037
-400.315054	12.155289	7.875034
-398.272020	2.352747	7.885030
-396.356558	15.581139	7.895027
-394.393010	18.482311	7.905024
-392.561550	10.815034	7.915021
-390.750973	21.349248	7.925018
-389.115659	7.072526	7.935014
-387.051737	11.228674	7.945011
-385.306772	17.137779	7.955008
-383.170490	3.652625	7.965005
-381.258486	4.081618	7.975002
-379.421965	29.467372	7.984998
-378.049411	5.464077	7.994995
-375.526223	-10.751130	8.004992
-374.150559	21.868395	8.014989
-372.088936	4.136930	8.024986
-369.785869	26.269927	8.034982
-368.057873	20.256478	8.044979
-366.443809	42.287928	8.054976
-364.427305	34.278500	8.064973
-362.697243	32.595591	8.074970
-361.059142	23.214534	8.084966
-358.961567	7.703555	8.094963
-356.929224	12.640002	8.104960
-355.107188	6.576820	8.114957
-353.294537	12.320412	8.124954
-351.286338	14.753460	8.134950
-349.458731	11.400326	8.144947
-347.524417	6.977048	8.154944
-345.723351	7.147475	8.164941
-343.773079	20.305629	8.174938
-341.981219	5.085036	8.184934
-340.219992	10.574754	8.194931
-338.112680	7.791163	8.204928
-336.277801	19.444126	8.214925
-334.879462	-1.258665	8.224922
-332.985281	30.940269	8.234918
-330.511131	3.322343	8.244915
-328.570414	25.180086	8.254912
-327.193785	9.299493	8.264909
-325.154005	-6.077491	8.274906
-323.014923	9.576739	8.284902
-321.386382	4.408114	8.294899
-319.698707	21.236473	8.304896
-317.564418	3.832904	8.314893
-315.331330	1.073466	8.324890
-313.902683	14.482267	8.334886
-311.831844	-19.437268	8.344883
-310.462707	19.214661	8.354880
-308.246513	12.812289	8.364877
-306.252066	6.494262	8.374874
-304.422171	4.320220	8.384870
-302.703714	0.597718	8.394867
-300.632987	-1.002156	8.404864
-298.870086	0.356978	8.414861
-296.928290	2.912769	8.424858
-295.129124	15.616684	8.434854
-293.208802	-1.931122	8.444851
-291.527560	5.587627	8.454848
-289.447674	17.359412	8.464845
-287.255008	-22.746656	8.474842
-285.673422	23.064762	8.484838
-283.816563	-9.712255	8.494835
-282.113323	-8.357797	8.504832
-280.396066	8.582698	8.514829
-278.338899	10.900628	8.524826
-276.202353	0.920627	8.534822
-274.044508	4.098769	8.544819
-272.531208	-9.490536	8.554816
-270.713302	17.035073	8.564813
-268.816546	2.625116	8.574810
-267.369790	9.005045	8.584807
-264.579810	-10.781442	8.594803
-263.153476	-17.542417	8.604800
-261.408893	28.291977	8.614797
-259.473226	27.498395	8.624794
-257.401586	-14.910901	8.634791
-255.682443	8.257988	8.644787
-253.581440	-15.992539	8.654784
-251.875119	-22.382946	8.664781
-249.840411	24.466153	8.674778
-248.181404	2.747616	8.684775
-246.173649	12.017375	8.694771
-244.796229	8.527752	8.704768
-242.598665	-21.917907	8.714765
-240.593259	-8.957945	8.724762
-238.830777	1.639323	8.734759
-236.799354	-5.102951	8.744755
-234.965652	-10.327942	8.754752
-233.038692	-10.824863	8.764749
-231.482182	2.849361	8.774746
-229.433599	5.860252	8.784743
-227.473177	-28.035287	8.794739
-225.980017	8.114911	8.804736
-223.555938	-1.895143	8.814733
-221.861187	-9.786783	8.824730
-220.118696	-10.227414	8.834727
-218.240591	-0.166454	8.844723
-216.268629	0.238892	8.854720
-214.221614	-30.818995	8.864717
-212.614989	-37.517131	8.874714
-210.818220	16.189132	8.884711
-208.661564	-4.168851	8.894707
-206.888881	-3.458551	8.904704
-204.981502	-4.329677	8.914701
-203.140194	-8.125395	8.924698
-200.970079	0.400101	8.934695
-199.622317	3.306544	8.944691
-197.938343	8.537134	8.954688
-195.451569	4.954196	8.964685
-193.837619	14.507889	8.974682
-191.856775	-18.841464	8.984679
-190.078240	10.166182	8.994675
-188.060841	24.603725	9.004672
-186.272174	0.295686	9.014669
-184.517623	5.627123	9.024666
-182.440059	3.899946	9.034663
-180.637643	-1.848943	9.044659
-178.492517	9.519395	9.054656
-176.831607	4.699364	9.064653
-174.873240	-1.568595	9.074650
-173.217161	4.683262	9.084647
-171.802742	7.678556	9.094643
-169.569769	-0.911542	9.104640
-167.165867	-6.985331	9.114637
-165.513368	-4.978509	9.124634
-163.770120	-7.872801	9.134631
-161.859004	3.739721	9.144627
-159.977586	3.927465	9.154624
-158.197487	10.369539	9.164621
-156.231850	10.695422	9.174618
-154.371947	1.869609	9.184615
-152.418182	23.954391	9.194611
-150.835244	10.110866	9.204608
-148.723634	14.085944	9.214605
-147.018178	-8.544643	9.224602
-144.842047	13.162034	9.234599
-143.474799	11.983993	9.244595
-141.080779	-20.127100	9.254592
-139.381535	-19.692390	9.264589
-137.392695	24.483245	9.274586
-135.736744	13.241129	9.284583
-133.340869	-26.376248	9.294579
-132.019796	24.174082	9.304576
-130.156940	10.169070	9.314573
-127.898474	8.237820	9.324570
-126.211445	16.392070	9.334567
-124.211389	0.909451	9.344563
-122.548114	10.747421	9.354560
-120.590403	28.813358	9.364557
-118.787207	-8.743791	9.374554
-117.156691	0.491533	9.384551
-115.104716	-3.808239	9.394547
-112.963148	18.281349	9.404544
-111.290697	15.663637	9.414541
-109.173741	1.463377	9.424538
-107.643963	-4.720367	9.434535
-105.385306	25.579694	9.444531
-103.589556	26.636905	9.454528
-102.128708	31.661603	9.464525
-100.158669	-0.411867	9.474522
-97.744720	24.446284	9.484519
-95.968803	4.133315	9.494515
-94.289515	-14.653222	9.504512
-92.742088	25.146765	9.514509
-90.770097	19.803492	9.524506
-88.544223	-10.313475	9.534503
-86.831729	15.302337	9.544499
-84.880482	26.786973	9.554496
-83.142648	20.222687	9.564493
-80.965911	-17.539273	9.574490
-79.421906	22.777561	9.584487
-77.319423	25.145281	9.594483
-75.905972	5.396964	9.604480
-73.608755	26.018680	9.614477
-71.641338	18.217827	9.624474
-70.255958	16.526953	9.634471
-68.221620	14.274682	9.644467
-65.698373	14.469059	9.654464
-64.477109	3.572635	9.664461
-62.784625	20.681495	9.674458
-60.513817	7.962978	9.684455
-58.803957	23.392299	9.694451
-56.554831	8.005771	9.704448
-54.950250	9.810324	9.714445
-52.832393	-6.829406	9.724442
-51.282931	40.474772	9.734439
-49.321822	4.656040	9.744435
-47.497705	35.161292	9.754432
-45.373372	-8.309465	9.764429
-43.620811	-3.217593	9.774426
-41.909244	21.020058	9.784423
-39.928601	20.933131	9.794419
-37.813070	6.955767	9.804416
-36.312911	7.600721	9.814413
-34.313222	-12.615261	9.824410
-32.625845	16.514469	9.834407
-30.640359	4.387783	9.844403
-28.215974	-17.774800	9.854400
-26.799366	23.615529	9.864397
-24.881293	11.775898	9.874394
-23.012842	0.207867	9.884391
-21.186229	27.494970	9.894387
-19.474921	16.940376	9.904384
-17.481394	7.679670	9.914381
-15.409015	14.165239	9.924378
-13.636498	1.919383	9.934375
-11.762694	32.868306	9.944371
-10.041365	11.004137	9.954368
-8.143515	5.598547	9.964365
-6.291478	13.115544	9.974362
-4.588207	-2.172823	9.984359
-3.316288	60.977221	9.994355
-2.125255	99.222306	10.004352
-0.943684	161.653016	10.014349
0.000000	226.763943	10.019354
0.835511	247.492981	10.024359
1.553985	333.863310	10.029363
1.483087	367.938908	10.034368
2.155563	353.393553	10.039373
2.592012	381.011270	10.044378
2.803586	442.486495	10.049383
3.294651	440.139030	10.054387
3.887811	432.855315	10.059392
3.728573	464.529401	10.064397
3.759693	507.285747	10.069402
3.743549	495.224921	10.074407
3.980332	486.594561	10.079411
3.830643	490.298993	10.084416
4.783818	476.404168	10.089421
4.404190	535.132474	10.094426
4.236606	542.627543	10.099431
4.294029	518.527770	10.104435
4.051720	527.542287	10.109440
4.943282	507.576648	10.114445
4.567707	501.245324	10.119450
4.773039	540.269800	10.124455
4.475598	559.167827	10.129459
4.392809	549.886666	10.134464
4.263985	537.933660	10.139469
5.047421	517.315061	10.144474
4.677376	502.604675	10.149479
4.976665	498.696675	10.154483
4.440317	550.610942	10.159488
4.528864	577.549674	10.164493
4.378104	575.511129	10.169498
5.116056	552.616343	10.174503
5.343079	590.691340	10.179507
5.119738	591.830843	10.184512
5.080969	566.178865	10.189517
5.374326	584.761931	10.194522
5.155419	602.505793	10.199527
5.543637	568.194598	10.204531
5.630633	596.257961	10.209536
5.227984	601.485080	10.214541
5.030516	584.290230	10.219546
5.544693	566.576630	10.224551
5.477263	565.937723	10.229555
5.314994	566.605444	10.234560
5.497959	564.644560	10.239565
5.357831	605.414773	10.244570
5.010186	636.548434	10.249575
5.572620	657.419386	10.254579
5.663218	662.840669	10.259584
5.764490	633.676476	10.264589
5.972126	607.840048	10.269594
5.881510	619.008169	10.274599
5.970017	665.649276	10.279603
6.084085	667.425670	10.284608
5.586662	651.764054	10.289613
5.447774	652.601512	10.294618
5.818048	647.934684	10.299623
6.433141	679.859476	10.304627
6.285153	715.353238	10.309632
6.688663	710.659012	10.314637
6.133468	695.373990	10.319642
6.506533	697.530124	10.324647
6.734375	701.226437	10.329651
6.311604	700.109613	10.334656
6.301310	709.872555	10.339661
6.509008	696.216265	10.344666
6.722776	670.910176	10.349671
6.644759	689.992572	10.354675
6.523983	692.847205	10.359680
7.122677	660.016087	10.364685
6.876886	664.480205	10.369690
6.786929	688.150237	10.374695
6.662017	725.504286	10.379699
6.502302	733.346702	10.384704
6.705379	714.419408	10.389709
6.759044	710.742913	10.394714
6.595898	722.556612	10.399719
6.665787	720.077581	10.404723
6.620610	725.000151	10.409728
6.822154	726.806755	10.414733
6.789597	732.247706	10.419738
6.728811	732.588591	10.424743
7.071012	741.002240	10.429747
6.840701	747.788332	10.434752
7.215886	745.506609	10.439757
7.830139	736.978325	10.444762
7.616823	792.891532	10.449767
7.764222	782.220486	10.454771
7.466842	769.100420	10.459776
7.874456	737.327774	10.464781
7.806054	744.296198	10.469786
7.641579	777.761636	10.474791
7.907786	754.020834	10.479795
7.365247	751.467586	10.484800
8.022076	726.305202	10.489805
7.863154	741.537057	10.494810
7.688543	773.174845	10.499815
7.920952	763.816468	10.504819
7.544310	776.272962	10.509824
7.802670	781.606033	10.514829
8.564921	763.658665	10.519834
8.352187	757.312295	10.524839
8.470014	785.311184	10.529843
8.242761	813.237429	10.534848
8.663029	808.941045	10.539853
8.509701	809.556888	10.544858
7.985979	774.807176	10.549863
8.303273	774.318212	10.554867
8.542177	756.348664	10.559872
8.596306	798.616500	10.564877
8.494599	806.946445	10.569882
8.380753	783.340326	10.574887
9.080522	788.871082	10.579891
8.572330	806.692869	10.584896
8.531950	777.341245	10.589901
8.628924	825.888048	10.594906
8.416964	795.045146	10.599911
8.816236	778.371480	10.604915
8.464595	826.594020	10.609920
8.578067	797.361320	10.614925
8.822647	789.205777	10.619930
8.127249	823.076116	10.624935
8.918663	787.951044	10.629939
8.971119	848.712204	10.634944
8.874001	836.585159	10.639949
9.852577	806.356604	10.644954
9.255782	811.118021	10.649959
9.353651	850.945795	10.654963
9.019884	836.486326	10.659968
9.163436	820.599297	10.664973
9.201391	857.913519	10.669978
9.267208	823.552215	10.674983
9.632219	850.198203	10.679987
9.424197	817.069614	10.684992
9.285857	845.303439	10.689997
9.448866	826.942208	10.695002
9.442179	868.065614	10.700007
9.494102	855.982593	10.705011
9.838954	851.797573	10.710016
10.033499	844.577230	10.715021
10.116541	895.823086	10.720026
9.590767	869.081292	10.725031
10.034818	869.264394	10.730035
10.016685	905.633623	10.735040
10.092547	884.286835	10.740045
9.567013	876.821772	10.745050
9.507183	879.393907	10.750055
9.518515	871.119399	10.755059
10.147156	865.359464	10.760064
10.366294	841.744298	10.765069
10.492472	853.411035	10.770074
10.077081	904.927228	10.775079
10.002235	905.699293	10.780083
9.605445	892.207037	10.785088
10.570725	877.223378	10.790093
10.922850	890.256026	10.795098
10.738419	939.223407	10.800103
10.759578	941.837829	10.805107
10.914331	926.166519	10.810112
10.746722	934.915482	10.815117
10.620519	906.704814	10.820122
10.430785	910.923521	10.825127
10.335034	908.999159	10.830131
10.705908	897.306785	10.835136
10.808568	880.774925	10.840141
10.776864	894.742430	10.845146
10.928506	934.115576	10.850151
10.906368	924.996390	10.855155
10.806181	918.745541	10.860160
11.255417	888.982864	10.865165
11.117868	886.555812	10.870170
11.073229	906.618770	10.875175
11.344542	936.528406	10.880179
11.284903	949.858593	10.885184
11.481586	930.809034	10.890189
11.416630	906.775443	10.895194
11.293472	927.962713	10.900199
11.227503	943.517426	10.905203
11.120911	943.286874	10.910208
11.982940	919.042343	10.915213
11.805505	935.310266	10.920218
11.533739	971.750075	10.925223
11.894597	961.735566	10.930227
12.098694	974.418157	10.935232
11.794541	932.263866	10.940237
11.870923	932.224907	10.945242
11.339051	957.675289	10.950247
11.682836	947.750247	10.955251
12.076735	926.956652	10.960256
12.327367	963.653750	10.965261
12.180979	956.203871	10.970266
12.441322	933.994948	10.975271
12.502338	935.142742	10.980275
11.911777	959.900738	10.985280
11.840726	926.688551	10.990285
12.185016	934.412847	10.995290
12.158275	978.914475	11.000295
12.332604	949.545606	11.005299
12.432179	976.972182	11.010304
12.225289	943.346378	11.015309
12.442667	975.188596	11.020314
12.199822	944.484343	11.025319
12.537096	975.115251	11.030323
12.014782	967.666974	11.035328
12.576079	926.475396	11.040333
12.681929	979.993474	11.045338
12.163206	957.282708	11.050343
13.082961	979.388678	11.055347
12.705541	1004.048100	11.060352
13.314442	968.070175	11.065357
12.894039	992.794781	11.070362
12.655640	974.994129	11.075367
12.983781	977.728334	11.080371
13.078992	984.760667	11.085376
13.003220	1004.120666	11.090381
13.329812	984.652919	11.095386
12.768307	1005.889712	11.100391
12.844191	985.738117	11.105395
12.992586	1034.946056	11.110400
13.090957	1004.046907	11.115405
13.405643	968.246793	11.120410
13.293882	1029.858080	11.125415
13.052128	1009.772881	11.130419
13.019544	1004.205082	11.135424
13.193215	1045.804860	11.140429
13.567817	1018.655835	11.145434
13.381129	1018.251973	11.150439
13.653339	1051.720938	11.155443
13.625040	1000.377553	11.160448
13.485989	1046.870096	11.165453
13.531227	1031.414838	11.170458
13.709961	1024.835603	11.175463
13.939868	1034.014820	11.180467
13.538807	1039.251302	11.185472
13.753245	1031.359056	11.190477
14.010465	1058.079389	11.195482
13.976190	1077.169511	11.200487
14.399427	1036.485351	11.205491
14.343577	1079.672001	11.210496
14.333378	1061.055818	11.215501
14.185411	1030.216401	11.220506
14.159263	1056.633413	11.225511
14.786938	1035.185781	11.230515
14.506080	1038.745689	11.235520
14.334033	1055.437094	11.240525
14.337307	1025.000928	11.245530
14.083354	1060.222269	11.250535
14.441610	1050.479356	11.255539
14.907602	1059.180960	11.260544
14.216311	1080.643568	11.265549
14.587475	1055.024697	11.270554
14.545199	1085.009884	11.275559
14.737492	1077.529583	11.280563
14.830696	1055.687759	11.285568
14.905085	1089.361828	11.290573
14.652668	1070.695953	11.295578
14.364333	1061.034076	11.300583
14.747405	1091.028711	11.305587
14.548932	1071.650896	11.310592
14.851639	1046.639057	11.315597
14.923396	1089.210862	11.320602
14.808492	1111.392160	11.325607
15.437131	1074.985037	11.330611
15.123955	1072.267413	11.335616
15.395862	1113.566284	11.340621
15.376113	1083.639880	11.345626
15.108303	1111.620476	11.350631
14.986536	1085.275905	11.355635
15.412209	1091.235278	11.360640
15.144692	1122.454972	11.365645
15.312490	1093.165703	11.370650
15.102336	1127.083940	11.375655
15.796401	1115.535394	11.380659
15.687287	1138.762929	11.385664
15.951020	1124.931717	11.390669
15.952846	1131.059631	11.395674
16.075677	1133.075965	11.400679
15.765652	1110.850501	11.405683
15.504228	1131.609101	11.410688
15.803704	1105.359741	11.415693
15.598791	1144.840788	11.420698
15.964810	1103.698778	11.425703
16.157310	1133.963597	11.430707
15.720130	1148.494341	11.435712
16.152324	1116.343201	11.440717
16.173117	1114.603654	11.445722
16.033208	1162.392986	11.450727
15.973954	1130.943104	11.455731
16.511543	1101.145401	11.460736
16.252145	1142.156921	11.465741
15.905383	1135.082690	11.470746
16.363713	1134.533375	11.475751
16.556395	1175.572239	11.480755
16.573867	1140.807876	11.485760
16.754440	1181.779302	11.490765
16.588218	1151.585951	11.495770
16.611922	1160.167339	11.500775
16.730667	1185.561666	11.505779
16.988861	1161.711087	11.510784
16.911072	1174.303189	11.515789
17.200314	1163.563509	11.520794
17.040435	1172.863328	11.525799
17.174361	1138.428914	11.530803
16.851146	1186.515647	11.535808
16.864894	1143.892136	11.540813
17.175155	1172.506071	11.545818
16.975907	1165.345219	11.550823
17.065713	1151.109625	11.555827
16.980332	1169.066278	11.560832
17.103632	1163.006767	11.565837
16.973907	1158.536217	11.570842
17.066001	1176.434612	11.575847
17.552707	1159.905842	11.580851
17.045569	1177.308434	11.585856
17.188197	1148.101918	11.590861
17.181685	1196.327414	11.595866
17.520982	1183.403483	11.600871
17.397922	1205.661921	11.605875
17.252572	1203.996171	11.610880
17.299479	1198.291038	11.615885
17.324127	1202.986585	11.620890
17.256352	1186.901040	11.625895
18.030524	1235.680267	11.630899
17.769209	1199.797977	11.635904
17.833132	1235.828509	11.640909
18.427684	1219.172084	11.645914
17.986984	1216.927368	11.650919
18.019665	1214.362721	11.655923
17.865273	1210.437000	11.660928
18.207919	1230.498566	11.665933
18.216874	1244.239931	11.670938
18.275449	1231.904004	11.675943
18.165739	1233.933784	11.680947
18.557869	1231.808563	11.685952
18.253594	1229.097374	11.690957
18.479286	1236.083788	11.695962
18.632587	1239.812629	11.700967
18.768455	1233.128170	11.705971
18.720691	1216.184668	11.710976
18.712407	1209.397050	11.715981
18.586292	1220.323706	11.720986
18.221727	1205.840393	11.725991
18.648632	1211.178283	11.730995
18.502550	1219.212758	11.736000
18.692151	1236.688810	11.741005
18.706526	1239.763276	11.746010
18.786346	1238.205118	11.751015
19.051028	1229.084154	11.756019
19.048667	1247.695522	11.761024
19.055313	1226.878891	11.766029
18.734824	1227.863618	11.771034
18.617256	1241.798629	11.776039
19.233311	1231.851261	11.781043
18.968657	1240.306792	11.786048
19.076471	1238.072368	11.791053
19.038216	1244.778384	11.796058
19.150942	1242.467480	11.801063
19.538652	1261.774405	11.806067
19.545513	1272.550579	11.811072
19.541353	1271.789581	11.816077
19.770071	1254.552774	11.821082
19.331988	1250.792137	11.826087
19.508375	1256.373431	11.831091
19.372254	1264.045208	11.836096
19.266504	1277.260043	11.841101
19.265633	1280.109860	11.846106
19.361845	1273.357588	11.851111
19.635951	1259.780069	11.856115
19.263327	1283.283256	11.861120
19.632945	1293.175241	11.866125
19.905259	1290.906689	11.871130
19.960721	1301.703519	11.876135
19.888051	1306.536050	11.881139
20.162969	1290.501396	11.886144
20.171156	1305.407559	11.891149
20.009084	1309.431152	11.896154
20.291014	1282.774248	11.901159
20.575070	1305.683871	11.906163
20.320799	1311.907900	11.911168
20.536050	1296.661797	11.916173
20.436070	1296.223596	11.921178
20.495927	1301.588518	11.926183
20.528904	1296.120542	11.931187
20.261161	1300.659318	11.936192
20.412445	1311.131780	11.941197
20.928038	1306.096205	11.946202
20.579866	1308.504658	11.951207
20.817378	1292.677824	11.956211
20.713898	1297.542075	11.961216
20.758210	1300.679590	11.966221
20.736856	1292.824807	11.971226
20.566779	1324.936174	11.976231
20.749370	1292.884378	11.981235
20.358189	1321.175221	11.986240
20.660607	1285.573410	11.991245
20.601457	1310.431758	11.996250
20.468592	1307.030874	12.001255
21.039739	1313.579019	12.006259
20.815404	1364.060237	12.011264
20.941680	1326.489919	12.016269
21.267823	1340.878616	12.021274
20.932857	1351.512237	12.026279
21.789940	1309.078608	12.031283
21.352653	1349.522974	12.036288
21.567299	1345.017946	12.041293
21.421790	1319.033140	12.046298
21.193757	1351.792498	12.051303
21.565231	1344.147861	12.056307
21.015721	1349.613139	12.061312
21.408567	1315.725236	12.066317
21.378821	1340.227274	12.071322
21.186682	1344.381832	12.076327
20.934855	1343.218766	12.081331
21.307552	1344.769488	12.086336
21.478253	1341.782246	12.091341
21.553399	1338.715624	12.096346
21.497335	1352.759997	12.101351
21.803814	1293.822490	12.106355
21.244231	1331.734716	12.111360
21.341171	1306.695320	12.116365
21.516021	1306.016162	12.121370
21.257928	1303.296017	12.126375
21.134906	1298.483721	12.131379
21.380338	1305.031766	12.136384
21.371518	1322.381867	12.141389
21.191286	1297.446617	12.146394
21.414279	1292.571255	12.151399
21.462233	1315.971149	12.156403
21.179270	1305.511862	12.161408
21.035775	1324.353214	12.166413
21.520781	1306.737991	12.171418
21.496610	1331.387363	12.176423
21.695186	1291.077378	12.181427
21.765350	1284.509034	12.186432
21.357918	1309.183221	12.191437
21.116165	1302.576301	12.196442
21.139565	1258.829660	12.201447
21.531316	1283.071986	12.206451
20.902162	1301.178604	12.211456
21.504675	1270.026593	12.216461
21.070373	1299.811386	12.221466
20.955931	1275.862349	12.226471
21.318902	1327.751084	12.231475
21.219468	1312.979366	12.236480
21.240335	1320.949423	12.241485
21.336859	1298.994735	12.246490
21.236190	1326.606878	12.251495
21.214551	1292.176408	12.256499
21.158663	1315.775796	12.261504
21.510635	1277.524612	12.266509
21.469642	1301.881718	12.271514
21.136315	1316.168976	12.276519
21.114217	1271.385575	12.281523
21.091166	1311.524067	12.286528
21.150515	1285.740047	12.291533
21.326295	1291.017090	12.296538
21.488627	1314.215807	12.301543
21.433213	1312.543586	12.306547
21.049333	1295.394967	12.311552
21.176326	1299.706781	12.316557
21.216042	1304.898292	12.321562
21.134227	1289.212278	12.326567
21.241643	1304.769689	12.331571
21.225180	1304.236164	12.336576
21.084693	1302.561742	12.341581
21.231776	1303.440365	12.346586
21.170651	1299.373584	12.351591
21.569612	1324.967901	12.356595
21.297708	1300.206544	12.361600
21.509463	1266.935859	12.366605
21.169240	1289.216443	12.371610
21.164404	1328.765432	12.376615
21.306469	1304.102057	12.381619
21.097041	1276.753948	12.386624
21.137404	1311.654561	12.391629
21.435620	1276.285263	12.396634
21.045847	1328.219930	12.401639
21.170510	1290.637345	12.406643
21.146278	1277.321861	12.411648
21.159530	1328.749117	12.416653
21.221288	1294.404693	12.421658
21.350069	1327.925558	12.426663
21.425061	1307.904550	12.431667
21.213750	1294.458032	12.436672
21.091368	1310.772790	12.441677
21.043212	1279.689834	12.446682
21.010748	1319.359902	12.451687
21.066154	1331.468835	12.456691
21.517221	1323.537116	12.461696
21.384908	1348.762025	12.466701
21.627284	1301.014152	12.471706
21.307077	1334.707566	12.476711
21.506005	1300.002195	12.481715
20.775752	1317.834788	12.486720
21.258411	1291.499105	12.491725
21.468589	1313.404932	12.496730
21.112214	1291.412094	12.501735
21.194699	1309.143446	12.506739
21.104524	1298.757500	12.511744
20.979385	1318.023284	12.516749
21.191242	1285.824906	12.521754
20.934611	1338.589958	12.526759
21.674933	1315.928576	12.531763
21.352906	1347.468117	12.536768
21.200629	1305.958746	12.541773
21.376028	1304.446841	12.546778
21.201747	1335.560657	12.551783
21.221462	1293.714796	12.556787
21.212028	1298.489929	12.561792
21.181797	1342.141644	12.566797
21.083892	1316.461500	12.571802
20.587638	1314.895856	12.576807
21.358651	1305.884911	12.581811
21.413859	1339.163637	12.586816
21.599357	1355.498732	12.591821
21.515143	1301.706214	12.596826
21.186842	1336.615218	12.601831
21.069727	1322.854019	12.606835
21.367102	1308.399081	12.611840
20.891890	1320.373424	12.616845
20.908345	1308.019707	12.621850
21.359896	1337.410977	12.626855
21.464181	1330.706279	12.631859
21.605207	1346.901795	12.636864
21.433563	1332.278773	12.641869
21.276668	1306.358886	12.646874
21.017014	1328.103113	12.651879
21.444289	1303.430525	12.656883
21.135448	1313.765052	12.661888
21.586217	1312.423703	12.666893
21.612376	1340.611754	12.671898
21.374762	1301.953046	12.676903
21.531097	1308.456954	12.681907
21.537749	1328.143295	12.686912
21.176248	1311.461036	12.691917
21.843679	1298.576139	12.696922
21.566428	1345.752444	12.701927
21.681071	1290.206157	12.706931
21.163915	1258.926798	12.711936
20.942322	1253.693408	12.716941
21.003695	1288.680505	12.721946
20.666686	1306.093965	12.726951
21.383246	1282.603764	12.731955
21.488322	1336.082278	12.736960
21.467980	1313.190539	12.741965
21.455600	1316.289788	12.746970
20.905035	1288.981869	12.751975
20.902672	1302.684880	12.756979
21.241858	1293.627691	12.761984
21.437659	1315.220412	12.766989
21.600821	1286.827232	12.771994
21.056797	1325.721012	12.776999
21.377769	1291.472454	12.782003
21.319988	1281.111318	12.787008
21.069404	1291.567430	12.792013
21.425347	1285.357222	12.797018
20.948695	1276.187296	12.802023
21.268198	1314.140633	12.807027
21.375714	1295.172628	12.812032
21.338541	1311.286133	12.817037
21.243338	1295.015602	12.822042
20.865406	1288.498218	12.827047
21.375228	1298.347346	12.832051
21.272523	1315.540517	12.837056
21.222030	1287.998300	12.842061
21.563600	1307.247987	12.847066
21.195623	1305.288136	12.852071
21.542193	1285.044069	12.857075
21.197349	1292.228737	12.862080
21.374977	1297.161700	12.867085
21.722629	1288.782853	12.872090
21.387507	1289.829844	12.877095
21.556524	1275.892165	12.882099
21.424725	1290.516277	12.887104
21.381568	1296.053750	12.892109
21.568464	1275.895087	12.897114
21.118523	1282.725916	12.902119
21.256098	1286.961919	12.907123
21.360394	1288.832992	12.912128
21.470491	1274.549886	12.917133
21.362493	1285.030563	12.922138
21.025281	1280.652992	12.927143
21.330170	1269.544874	12.932147
21.230399	1282.291967	12.937152
21.046735	1274.833676	12.942157
21.342834	1268.451663	12.947162
21.476065	1298.912366	12.952167
21.205602	1287.927533	12.957171
20.928678	1269.546015	12.962176
21.101617	1291.402552	12.967181
21.245132	1287.867706	12.972186
21.387772	1277.064588	12.977191
21.254829	1315.519030	12.982195
21.161733	1299.738607	12.987200
21.427696	1299.732493	12.992205
21.453427	1312.609414	12.997210
20.978755	1282.024998	13.002215
21.770881	1255.759878	13.007219
21.164493	1266.378375	13.012224
20.786560	1291.781134	13.017229
21.451812	1257.641758	13.022234
21.114474	1280.462779	13.027239
21.051220	1309.084513	13.032243
21.098573	1283.062705	13.037248
21.599147	1286.054909	13.042253
21.399410	1309.087427	13.047258
21.270629	1311.773140	13.052263
20.633647	1280.361452	13.057267
21.144230	1254.682147	13.062272
21.253295	1286.155958	13.067277
21.206309	1298.722755	13.072282
21.083919	1327.327146	13.077287
21.256370	1324.144080	13.082291
20.936686	1305.485475	13.087296
21.036971	1271.694797	13.092301
21.327133	1311.135189	13.097306
20.886175	1315.405117	13.102311
21.666657	1272.406626	13.107315
21.646289	1319.529262	13.112320
21.194912	1319.941914	13.117325
21.468699	1294.576280	13.122330
21.374690	1307.186854	13.127335
21.463549	1331.220514	13.132339
20.958419	1290.313107	13.137344
21.380296	1292.234460	13.142349
21.609584	1295.008149	13.147354
21.273484	1282.806876	13.152359
21.468756	1264.689114	13.157363
21.258083	1296.925169	13.162368
20.996273	1285.106298	13.167373
21.559178	1256.267791	13.172378
21.234015	1268.006844	13.177383
21.081336	1288.488119	13.182387
21.453142	1270.518820	13.187392
21.320668	1275.118020	13.192397
21.529742	1282.737908	13.197402
21.294613	1267.322382	13.202407
21.310679	1293.614818	13.207411
21.362710	1262.960635	13.212416
21.079731	1295.492079	13.217421
21.527786	1261.433066	13.222426
21.484191	1299.553086	13.227431
21.127762	1278.869191	13.232435
21.244444	1287.754382	13.237440
21.285746	1275.809904	13.242445
21.285974	1269.629624	13.247450
21.268655	1278.985625	13.252455
21.553197	1263.105590	13.257459
21.608861	1269.914126	13.262464
21.394384	1287.044663	13.267469
21.331444	1247.670667	13.272474
21.135614	1278.287888	13.277479
21.212826	1231.578231	13.282483
21.049067	1262.708349	13.287488
21.119745	1256.589381	13.292493
21.389616	1293.628034	13.297498
20.844951	1272.111547	13.302503
21.154080	1284.042777	13.307507
21.691828	1276.133530	13.312512
20.914526	1296.504692	13.317517
21.526170	1267.475457	13.322522
21.611096	1274.143706	13.327527
21.078041	1275.547126	13.332531
20.943678	1244.951094	13.337536
21.248943	1297.110706	13.342541
21.398339	1262.566293	13.347546
21.289194	1291.972774	13.352551
21.334986	1273.225960	13.357555
20.878023	1258.779407	13.362560
20.896934	1272.168328	13.367565
21.441966	1292.505219	13.372570
21.594468	1280.263874	13.377575
21.079167	1292.824926	13.382579
21.148302	1274.310939	13.387584
21.001199	1293.709508	13.392589
21.208908	1280.071594	13.397594
20.919437	1278.245887	13.402599
21.324416	1287.354767	13.407603
21.411788	1301.365175	13.412608
21.178392	1275.957454	13.417613
21.329660	1302.414430	13.422618
21.484383	1288.035880	13.427623
21.165631	1297.427351	13.432627
21.393752	1282.327448	13.437632
21.117847	1285.725771	13.442637
21.177917	1296.906652	13.447642
21.068780	1284.561945	13.452647
21.081431	1300.069807	13.457651
21.194098	1295.394972	13.462656
21.043196	1278.810055	13.467661
21.481857	1305.634378	13.472666
20.867508	1291.488869	13.477671
21.443822	1293.891812	13.482675
21.292807	1273.794928	13.487680
21.070988	1295.911554	13.492685
21.515460	1284.468916	13.497690
21.481692	1284.373405	13.502695
21.438490	1294.889489	13.507699
21.566312	1281.986582	13.512704
21.357058	1280.154390	13.517709
21.158503	1284.209026	13.522714
21.206358	1277.068636	13.527719
21.302898	1278.414225	13.532723
21.079224	1292.292876	13.537728
21.403045	1285.647806	13.542733
21.267109	1274.621027	13.547738
21.072827	1268.519078	13.552743
21.367557	1277.714922	13.557747
21.106789	1291.325089	13.562752
21.144088	1289.130289	13.567757
21.510841	1284.955848	13.572762
21.243827	1268.744286	13.577767
21.249067	1272.156117	13.582771
21.155596	1271.675877	13.587776
21.122806	1257.822441	13.592781
21.490024	1283.634643	13.597786
21.360544	1267.737050	13.602791
21.191821	1260.967110	13.607795
21.276030	1272.402751	13.612800
21.008138	1267.343903	13.617805
21.505107	1256.156274	13.622810
20.990696	1280.872706	13.627815
21.270787	1257.004286	13.632819
21.071679	1263.124877	13.637824
21.084354	1295.782640	13.642829
21.656059	1268.343087	13.647834
21.214149	1294.923036	13.652839
21.372520	1255.374949	13.657843
21.382178	1281.556418	13.662848
21.091756	1261.527517	13.667853
21.308091	1254.462773	13.672858
21.242833	1279.982808	13.677863
21.333878	1251.598045	13.682867
21.472764	1279.629224	13.687872
21.268808	1253.811556	13.692877
21.514538	1286.916271	13.697882
21.217887	1251.772794	13.702887
21.171501	1286.754993	13.707891
21.116179	1261.620105	13.712896
21.174374	1264.592967	13.717901
20.872726	1287.354690	13.722906
20.890383	1264.587859	13.727911
21.668986	1242.849338	13.732915
21.126629	1291.493356	13.737920
20.756413	1270.830596	13.742925
21.280939	1257.172139	13.747930
20.990213	1276.890067	13.752935
21.525113	1291.709062	13.757939
21.309506	1279.860749	13.762944
21.653345	1272.348294	13.767949
21.474170	1266.682344	13.772954
21.240657	1280.736023	13.777959
21.492381	1247.060027	13.782963
21.460992	1293.693890	13.787968
21.200349	1266.603135	13.792973
21.550281	1267.044114	13.797978
21.543149	1268.332118	13.802983
21.595016	1264.934899	13.807987
21.572742	1273.205132	13.812992
21.433067	1258.023559	13.817997
21.477854	1233.433378	13.823002
21.006794	1262.442554	13.828007
21.415153	1222.235714	13.833011
20.880700	1256.449619	13.838016
20.949312	1238.728204	13.843021
21.414173	1268.822921	13.848026
21.474639	1272.038280	13.853031
21.213943	1256.076469	13.858035
21.124111	1258.675533	13.863040
20.863815	1235.969633	13.868045
20.979342	1276.067792	13.873050
20.958267	1262.879556	13.878055
21.299411	1268.041905	13.883059
20.950527	1296.081519	13.888064
21.149520	1258.821487	13.893069
21.150995	1247.067894	13.898074
21.128797	1293.279231	13.903079
20.987387	1281.955265	13.908083
21.394957	1257.675416	13.913088
21.379034	1278.420305	13.918093
21.278319	1287.687106	13.923098
21.185604	1273.784863	13.928103
21.111831	1292.564590	13.933107
21.110800	1273.560306	13.938112
21.370400	1273.372275	13.943117
21.353547	1277.112493	13.948122
21.144020	1264.645038	13.953127
21.313311	1277.298752	13.958131
21.131338	1280.783021	13.963136
21.418744	1243.376460	13.968141
21.352439	1292.580090	13.973146
21.185875	1273.944416	13.978151
21.468685	1268.053394	13.983155
21.369518	1286.025006	13.988160
21.563351	1267.631493	13.993165
21.607807	1300.016107	13.998170
21.336246	1312.790625	14.003175
21.324231	1285.876232	14.008179
21.625777	1252.826233	14.013184
21.392090	1274.509467	14.018189
21.105888	1251.793192	14.023207
20.793573	1236.725149	14.028224
20.924166	1281.610539	14.033242
21.365811	1254.394438	14.038259
21.129489	1256.431415	14.043277
21.222719	1290.580925	14.048295
21.405990	1264.223963	14.053312
21.267830	1296.307316	14.058330
21.244947	1266.382670	14.063347
21.271741	1283.641104	14.068365
21.236870	1259.635941	14.073383
21.018007	1301.341508	14.078400
21.437942	1272.735171	14.083418
21.138957	1286.448159	14.088435
21.484252	1270.522531	14.093453
21.247026	1297.193333	14.098471
21.341268	1272.258374	14.103488
21.457613	1292.201770	14.108506
21.686434	1300.914240	14.113523
21.287949	1276.810527	14.118541
21.622288	1325.241304	14.123559
21.466610	1310.395162	14.128576
21.851748	1307.573184	14.133594
21.691445	1326.674372	14.138611
21.561962	1313.772978	14.143629
21.602384	1309.159292	14.148647
21.722476	1327.098944	14.153664
21.607228	1318.344814	14.158682
22.088346	1310.917558	14.163699
21.609816	1335.847083	14.168717
21.684357	1315.046644	14.173735
21.773288	1304.281145	14.178752
21.683315	1308.660556	14.183770
21.931780	1331.691940	14.188787
21.503422	1297.746063	14.193805
22.028707	1336.054168	14.198823
21.831432	1307.090819	14.203840
21.709928	1333.528519	14.208858
21.393261	1327.501034	14.213875
21.679173	1315.834250	14.218893
22.026385	1317.823789	14.223911
21.771811	1342.613790	14.228928
21.589491	1305.685596	14.233946
22.179927	1321.200192	14.238963
22.000960	1322.048291	14.243981
21.946831	1343.139697	14.248999
21.876841	1336.833773	14.254016
22.040612	1338.799089	14.259034
21.900128	1360.933026	14.264051
22.249097	1349.240430	14.269069
22.158668	1348.186824	14.274087
22.084592	1360.315405	14.279104
22.046961	1352.736484	14.284122
22.263079	1377.023624	14.289139
22.331177	1342.721620	14.294157
21.939734	1380.191353	14.299175
21.987725	1387.373878	14.304192
22.348021	1354.845198	14.309210
22.389779	1348.206849	14.314227
21.863132	1387.261713	14.319245
22.106677	1357.746624	14.324263
22.082451	1365.368510	14.329280
21.974759	1352.510797	14.334298
22.229756	1365.647095	14.339315
22.315008	1360.456821	14.344333
22.168399	1366.155583	14.349351
22.024720	1371.087832	14.354368
22.226379	1386.670793	14.359386
22.795128	1392.190985	14.364403
22.727744	1389.282289	14.369421
22.796057	1390.164886	14.374439
22.670804	1374.527329	14.379456
22.284414	1363.928825	14.384474
22.413702	1371.611173	14.389491
22.635606	1383.459767	14.394509
22.760084	1384.959457	14.399527
22.685102	1410.707200	14.404544
22.995426	1377.975656	14.409562
22.553757	1364.192795	14.414579
22.283529	1380.862439	14.419597
23.101688	1374.622490	14.424615
23.034027	1362.337244	14.429632
22.697145	1364.890484	14.434650
22.456301	1377.448361	14.439667
22.594331	1355.966071	14.444685
22.867449	1384.505362	14.449703
22.970169	1395.707598	14.454720
23.052722	1382.361777	14.459738
23.177812	1378.038153	14.464755
22.605578	1377.177786	14.469773
22.592917	1352.581415	14.474791
22.789708	1376.764674	14.479808
22.574932	1395.132187	14.484826
22.797991	1380.739941	14.489843
22.612952	1394.460811	14.494861
23.083890	1395.117179	14.499879
22.626253	1389.607643	14.504896
23.031880	1361.869346	14.509914
23.015893	1409.662587	14.514931
22.809813	1378.117642	14.519949
22.490946	1403.581804	14.524967
22.909346	1382.205768	14.529984
23.097752	1419.093925	14.535002
23.521050	1409.892063	14.540019
22.934693	1420.631643	14.545037
23.435650	1399.072533	14.550055
23.091418	1406.638512	14.555072
23.281409	1420.309035	14.560090
23.480706	1416.207942	14.565107
23.013492	1403.165280	14.570125
23.409340	1420.859726	14.575143
23.516261	1403.654585	14.580160
23.055888	1397.392018	14.585178
23.158091	1409.377698	14.590195
23.175539	1395.488553	14.595213
23.195902	1444.532932	14.600231
23.325298	1409.195400	14.605248
23.415283	1432.345025	14.610266
23.593827	1402.135510	14.615283
23.098750	1436.206943	14.620301
23.503152	1412.777188	14.625319
23.728651	1426.528568	14.630336
23.600399	1412.981962	14.635354
23.503981	1428.349815	14.640371
23.547236	1401.075068	14.645389
23.499276	1409.144346	14.650407
23.359577	1423.965403	14.655424
23.856224	1395.468499	14.660442
23.806640	1428.040588	14.665459
23.412523	1435.268478	14.670477
23.752739	1408.679375	14.675495
23.875855	1402.449589	14.680512
23.704785	1448.880310	14.685530
23.491632	1420.704193	14.690547
23.809959	1401.565160	14.695565
23.776415	1431.875880	14.700583
23.595005	1420.502189	14.705600
23.825829	1401.694856	14.710618
23.829215	1436.053302	14.715635
23.756878	1417.382386	14.720653
24.040879	1392.700883	14.725671
23.926597	1436.358759	14.730688
23.397466	1428.962001	14.735706
23.820000	1392.753508	14.740723
23.476707	1447.877315	14.745741
23.539160	1436.823363	14.750759
23.917205	1431.287499	14.755776
24.188865	1441.223305	14.760794
24.274530	1467.247543	14.765811
24.331718	1428.659075	14.770829
24.187595	1461.200699	14.775847
23.904049	1425.796851	14.780864
24.280231	1441.454282	14.785882
24.516594	1449.767670	14.790899
24.511416	1394.240180	14.795917
24.428008	1433.977945	14.800935
24.427387	1400.935722	14.805952
24.251433	1438.847857	14.810970
24.622611	1398.411456	14.815987
24.295390	1436.528603	14.821005
24.087667	1422.164119	14.826023
24.436518	1386.167164	14.831040
24.199925	1435.137663	14.836058
24.239294	1401.505480	14.841075
24.334496	1428.998878	14.846093
24.296072	1412.823625	14.851111
24.375983	1425.523867	14.856128
24.161814	1420.925580	14.861146
24.670355	1417.272235	14.866163
24.308657	1404.764865	14.871181
24.247563	1416.815919	14.876199
24.499499	1400.308087	14.881216
24.147363	1424.745707	14.886234
24.631530	1424.957955	14.891251
24.403940	1432.123106	14.896269
24.770554	1452.482193	14.901287
24.901331	1432.198000	14.906304
24.182091	1452.012971	14.911322
24.518532	1417.677432	14.916339
24.650473	1467.874406	14.921357
24.420753	1432.959024	14.926375
24.589506	1465.342223	14.931392
24.758486	1433.705882	14.936410
24.744243	1443.342799	14.941427
24.508512	1448.148186	14.946445
24.521266	1447.494962	14.951463
24.961857	1445.161183	14.956480
24.678785	1449.445592	14.961498
24.695668	1462.129177	14.966515
24.811095	1444.283994	14.971533
24.488247	1451.283451	14.976551
24.891521	1447.936319	14.981568
24.451079	1444.528692	14.986586
24.913771	1483.404011	14.991603
24.879433	1454.916169	14.996621
24.843050	1494.424806	15.001639
25.139610	1498.475219	15.006656
24.732656	1483.513246	15.011674
25.452839	1448.185218	15.016691
25.045138	1490.681988	15.021709
25.187376	1465.277367	15.026727
25.342154	1474.752072	15.031744
25.083695	1487.051734	15.036762
25.316579	1466.351667	15.041779
25.338301	1480.275594	15.046797
25.446671	1469.448672	15.051815
25.666678	1464.587649	15.056832
25.501139	1500.187544	15.061850
25.874995	1456.923864	15.066867
25.538236	1449.483831	15.071885
25.210239	1464.281477	15.076903
25.812575	1444.648788	15.081920
25.213499	1442.804853	15.086938
25.469612	1443.239086	15.091955
25.288048	1454.137499	15.096973
25.576267	1445.111312	15.101991
25.534573	1427.767825	15.107008
25.095801	1453.664895	15.112026
25.597292	1433.757298	15.117043
25.460798	1443.718875	15.122061
25.655209	1421.308865	15.127079
25.484210	1446.812440	15.132096
25.283500	1446.311234	15.137114
25.139575	1438.142042	15.142131
24.881387	1472.073536	15.147149
25.125098	1471.704370	15.152167
25.597004	1456.213733	15.157184
25.304311	1483.644829	15.162202
25.704037	1469.759141	15.167219
25.671505	1477.717459	15.172237
25.277033	1465.882216	15.177255
25.972890	1496.805046	15.182272
25.770767	1503.341688	15.187290
25.991432	1486.461224	15.192307
26.033610	1507.353468	15.197325
25.973492	1495.881724	15.202343
25.997119	1470.182983	15.207360
25.645547	1490.085659	15.212378
26.161705	1482.246894	15.217395
26.322399	1477.860935	15.222413
25.962207	1483.883237	15.227431
26.002203	1466.444880	15.232448
25.629180	1468.642111	15.237466
26.135249	1477.313617	15.242483
26.315297	1484.015814	15.247501
25.912689	1499.198196	15.252519
26.631397	1485.708354	15.257536
25.988176	1479.721872	15.262554
26.052056	1468.955528	15.267571
26.515282	1475.192568	15.272589
26.297541	1472.328283	15.277607
26.583865	1472.298382	15.282624
26.371213	1469.071495	15.287642
26.249350	1461.760776	15.292659
26.220899	1464.760339	15.297677
26.025594	1469.537263	15.302695
26.776290	1471.257986	15.307712
26.272310	1458.798428	15.312730
26.147560	1459.535643	15.317747
26.265395	1480.903414	15.322765
26.298000	1501.605270	15.327783
26.406060	1492.474080	15.332800
26.369377	1492.028510	15.337818
26.531679	1495.003950	15.342835
26.461335	1492.904228	15.347853
26.240982	1523.386502	15.352871
26.805139	1479.562302	15.357888
26.481796	1514.243597	15.362906
26.476722	1489.172310	15.367923
26.695979	1509.940364	15.372941
26.736394	1495.540953	15.377959
26.603561	1497.503256	15.382976
26.402552	1502.350313	15.387994
26.755393	1499.503563	15.393011
26.965002	1495.704394	15.398029
26.711303	1509.357672	15.403047
26.794310	1503.900294	15.408064
26.578566	1486.987183	15.413082
26.386046	1526.730019	15.418099
27.100314	1501.602191	15.423117
26.789659	1512.159443	15.428135
26.864649	1511.501010	15.433152
26.938350	1517.694799	15.438170
26.976860	1523.326347	15.443187
27.386959	1529.243125	15.448205
26.976267	1513.809814	15.453223
27.097264	1503.448036	15.458240
27.126745	1503.166517	15.463258
27.278489	1501.323955	15.468275
27.603187	1482.341100	15.473293
26.995430	1513.231197	15.478311
26.980564	1487.076100	15.483328
27.146502	1498.015080	15.488346
26.836821	1499.749188	15.493363
27.352851	1505.581423	15.498381
27.150139	1520.354426	15.503399
27.385370	1502.225800	15.508416
27.261154	1531.542892	15.513434
27.377220	1527.426728	15.518451
27.621611	1527.258798	15.523469
27.421689	1504.740090	15.528487
27.311755	1500.170771	15.533504
27.294595	1515.453717	15.538522
27.341180	1497.830230	15.543539
27.552942	1537.302556	15.548557
27.275753	1509.399171	15.553575
27.331821	1543.533968	15.558592
27.554700	1509.832942	15.563610
27.297465	1542.314136	15.568627
27.394597	1528.924957	15.573645
27.577320	1518.105017	15.578663
27.758177	1533.379998	15.583680
27.665805	1537.714244	15.588698
27.429794	1512.321100	15.593715
27.753006	1542.125276	15.598733
27.557379	1511.874532	15.603751
27.602438	1527.175882	15.608768
28.040346	1519.126210	15.613786
27.891760	1513.115885	15.618803
27.560192	1546.785553	15.623821
27.662412	1518.340301	15.628839
27.522161	1546.236409	15.633856
27.705591	1528.222977	15.638874
27.655112	1565.824425	15.643891
28.164684	1545.932690	15.648909
27.731997	1574.842892	15.653927
28.318459	1536.419838	15.658944
28.553087	1544.923892	15.663962
28.529907	1544.836386	15.668979
28.364997	1528.045680	15.673997
28.201984	1535.321705	15.679015
28.316567	1507.738084	15.684032
28.254675	1519.772047	15.689050
27.951193	1508.436631	15.694067
28.234163	1514.719738	15.699085
28.308763	1524.449506	15.704103
28.322446	1517.491518	15.709120
28.243038	1502.183135	15.714138
27.724074	1527.113142	15.719155
28.229542	1517.114751	15.724173
28.322918	1527.785330	15.729191
28.382615	1524.584209	15.734208
28.517392	1526.407885	15.739226
28.245876	1541.336598	15.744243
28.617493	1527.192646	15.749261
28.135756	1552.047546	15.754279
28.623507	1551.751143	15.759296
28.876745	1551.652587	15.764314
28.485079	1522.081167	15.769331
28.800171	1520.107160	15.774349
28.641604	1524.319826	15.779367
28.669239	1518.264092	15.784384
28.602970	1511.213466	15.789402
28.430677	1519.079267	15.794419
28.678713	1531.760655	15.799437
28.519483	1538.202384	15.804455
28.772315	1550.964820	15.809472
28.981287	1543.237934	15.814490
28.873981	1555.502537	15.819507
28.906161	1551.133905	15.824525
29.085482	1547.919993	15.829543
29.478195	1532.430893	15.834560
28.814093	1509.078579	15.839578
28.686575	1514.005154	15.844595
29.051267	1504.232141	15.849613
28.508362	1510.327636	15.854631
29.022561	1529.964882	15.859648
29.235657	1534.357375	15.864666
28.558316	1531.066157	15.869683
28.880020	1541.116747	15.874701
28.758279	1548.312264	15.879719
29.095343	1541.214604	15.884736
29.206476	1551.921694	15.889754
28.875490	1549.193429	15.894771
29.329660	1539.777353	15.899789
28.933248	1541.885516	15.904807
29.012143	1551.230802	15.909824
29.525819	1548.397719	15.914842
29.212195	1546.300608	15.919859
29.168581	1537.986375	15.924877
29.213112	1540.620388	15.929895
29.321675	1550.324307	15.934912
29.662557	1549.689535	15.939930
29.562924	1554.001348	15.944947
29.423848	1549.499581	15.949965
29.565553	1543.277782	15.954983
29.319189	1542.137347	15.960000
29.460622	1542.449874	15.965018
29.669581	1566.582747	15.970035
29.332504	1557.160713	15.975053
29.640269	1566.291759	15.980071
29.844948	1565.071525	15.985088
29.732698	1570.130963	15.990106
29.704887	1583.182002	15.995123
29.929075	1565.873025	16.000141
29.578865	1553.080550	16.005159
29.658842	1563.237345	16.010176
29.672718	1563.334264	16.015194
29.850643	1564.687025	16.020211
29.940790	1566.783663	16.025229
29.595002	1564.435278	16.030247
29.614577	1574.266662	16.035264
29.975738	1572.296313	16.040282
29.882918	1580.981597	16.045299
29.891095	1557.872771	16.050317
29.922100	1574.878412	16.055335
29.741338	1579.654626	16.060352
30.148672	1575.078294	16.065370
29.835173	1567.892464	16.070387
29.829847	1564.019017	16.075405
29.523521	1596.174682	16.080423
30.268274	1567.743266	16.085440
30.341839	1594.963580	16.090458
30.291108	1607.228642	16.095475
30.242354	1595.679501	16.100493
30.365976	1588.691362	16.105511
30.312226	1578.590205	16.110528
30.598306	1575.271173	16.115546
29.854051	1576.610555	16.120563
30.296363	1579.042712	16.125581
30.114201	1598.185495	16.130599
30.541238	1599.272017	16.135616
30.596894	1596.071524	16.140634
30.629502	1604.524462	16.145651
30.677675	1594.292209	16.150669
30.821646	1607.905756	16.155687
30.571193	1598.262242	16.160704
30.788059	1592.048885	16.165722
30.929782	1585.801896	16.170739
31.063958	1562.823978	16.175757
30.965474	1564.168911	16.180775
30.904131	1560.672483	16.185792
31.197776	1552.016596	16.190810
30.714692	1558.078975	16.195827
30.689334	1553.942886	16.200845
30.504828	1557.042860	16.205863
30.523154	1552.846323	16.210880
30.421564	1567.471114	16.215898
30.670831	1569.720126	16.220915
30.883682	1573.264816	16.225933
30.740180	1596.283627	16.230951
31.067757	1599.893398	16.235968
31.130457	1599.491750	16.240986
30.967117	1599.911085	16.246003
31.049945	1588.605232	16.251021
30.891491	1603.663841	16.256039
30.934591	1593.770596	16.261056
31.072407	1588.545117	16.266074
31.266426	1592.457755	16.271091
30.909068	1605.185418	16.276109
31.419931	1594.379157	16.281127
31.110754	1585.539390	16.286144
31.110989	1598.957202	16.291162
31.135998	1599.330769	16.296179
31.235321	1576.501533	16.301197
31.481647	1610.151544	16.306215
31.143382	1585.378618	16.311232
31.479192	1587.536754	16.316250
31.086733	1597.116115	16.321267
31.444393	1596.783830	16.326285
31.342546	1598.324356	16.331303
31.419864	1589.245199	16.336320
31.895831	1601.923332	16.341338
31.347425	1599.190406	16.346355
31.584445	1606.528510	16.351373
31.997423	1600.757352	16.356391
31.453756	1598.190409	16.361408
31.437535	1599.803796	16.366426
31.269673	1624.218655	16.371443
31.722870	1622.411372	16.376461
31.776445	1619.915919	16.381479
31.571778	1644.987911	16.386496
31.913996	1627.641162	16.391514
31.705367	1618.303995	16.396531
31.452940	1618.997086	16.401549
31.852476	1618.897222	16.406567
31.797111	1625.935901	16.411584
32.058476	1607.411295	16.416602
31.745858	1639.294354	16.421619
32.525152	1609.981175	16.426637
32.106458	1616.443868	16.431655
31.757073	1623.211686	16.436672
32.321037	1617.677563	16.441690
31.924773	1618.322807	16.446707
32.057655	1623.023847	16.451725
32.754690	1627.726154	16.456743
32.140205	1629.587537	16.461760
32.223435	1625.020406	16.466778
31.921767	1628.066721	16.471795
32.316797	1636.021434	16.476813
32.244066	1637.532152	16.481831
32.270674	1653.852750	16.486848
32.591823	1647.614873	16.491866
32.631996	1653.178566	16.496883
32.639730	1656.458688	16.501901
33.075899	1636.374044	16.506919
32.798755	1641.447219	16.511936
32.896363	1610.197828	16.516954
32.166868	1611.196661	16.521971
32.125428	1628.976831	16.526989
32.726470	1611.352871	16.532007
32.175222	1614.144831	16.537024
32.370968	1615.442846	16.542042
32.634351	1653.867493	16.547059
32.789241	1641.143826	16.552077
32.566670	1637.009277	16.557095
32.629684	1653.275304	16.562112
32.867144	1642.806765	16.567130
32.680910	1649.743631	16.572147
32.736228	1638.484598	16.577165
32.585046	1659.667447	16.582183
32.700830	1642.515666	16.587200
33.234957	1640.557049	16.592218
32.912409	1644.621295	16.597235
32.850977	1638.809376	16.602253
32.964763	1635.706570	16.607271
33.025027	1663.487555	16.612288
33.052663	1632.939831	16.617306
32.913701	1669.896566	16.622323
33.048993	1672.171636	16.627341
33.301092	1661.567041	16.632359
33.251305	1668.725975	16.637376
33.501359	1657.545983	16.642394
33.458253	1674.176595	16.647411
33.465291	1669.939352	16.652429
33.869229	1660.729410	16.657447
33.701456	1654.388605	16.662464
33.640636	1637.851731	16.667482
33.373155	1644.203804	16.672499
33.717385	1640.960427	16.677517
33.856465	1636.274274	16.682535
33.372375	1640.172373	16.687552
33.780380	1633.371667	16.692570
33.736206	1641.822714	16.697587
33.320318	1646.479145	16.702605
33.709027	1635.849636	16.707623
33.285290	1649.948587	16.712640
33.340108	1640.671639	16.717658
33.283707	1656.627953	16.722675
33.510656	1658.411778	16.727693
34.107074	1661.272403	16.732711
33.789656	1671.031754	16.737728
33.828539	1667.528754	16.742746
34.022237	1657.238643	16.747763
33.918974	1659.698046	16.752781
33.828807	1660.684585	16.757799
33.828111	1665.716828	16.762816
34.099809	1664.605447	16.767834
34.122595	1668.348786	16.772851
33.870969	1665.370315	16.777869
34.237285	1656.833338	16.782887
33.805451	1666.052509	16.787904
33.848586	1664.680278	16.792922
34.068148	1672.758948	16.797939
33.893904	1670.100044	16.802957
34.212044	1679.448158	16.807975
34.381037	1696.793731	16.812992
34.562415	1684.352092	16.818010
34.191220	1691.090386	16.823027
34.057336	1694.633774	16.828045
34.546696	1684.585929	16.833063
34.353126	1690.389834	16.838080
34.224897	1675.567254	16.843098
34.660387	1690.808085	16.848115
34.331796	1697.899811	16.853133
35.023027	1679.575547	16.858151
34.735497	1682.009284	16.863168
34.980557	1680.848668	16.868186
34.669058	1688.983725	16.873203
34.713416	1686.983660	16.878221
34.985160	1690.704605	16.883239
34.647378	1681.104850	16.888256
34.786099	1690.434394	16.893274
35.080104	1687.368903	16.898291
35.020351	1693.706746	16.903309
35.110909	1676.815351	16.908327
35.018326	1676.562733	16.913344
35.183102	1675.806604	16.918362
34.840656	1661.026066	16.923379
34.984099	1679.121306	16.928397
35.051082	1677.130218	16.933415
34.831488	1677.052012	16.938432
35.012485	1679.884510	16.943450
34.883347	1690.930469	16.948467
35.326788	1685.555541	16.953485
35.124111	1680.662755	16.958503
34.777290	1681.084611	16.963520
34.764374	1685.036568	16.968538
34.696114	1688.344547	16.973555
34.886463	1686.804118	16.978573
35.349382	1699.677901	16.983591
35.340712	1725.365290	16.988608
35.309775	1697.839122	16.993626
35.678999	1724.090734	16.998643
35.086623	1732.844764	17.003661
35.432614	1697.549067	17.008679
35.224243	1692.710667	17.013696
35.314301	1745.156843	17.018714
35.418557	1723.432430	17.023731
35.052148	1709.443752	17.028749
35.938742	1717.200567	17.033767
36.085269	1744.096493	17.038784
36.008267	1737.379378	17.043802
36.003004	1706.468656	17.048819
35.657971	1736.018005	17.053837
35.440491	1703.343160	17.058855
35.714784	1715.451087	17.063872
36.016239	1739.064555	17.068890
36.509536	1725.511342	17.073907
35.663376	1733.019107	17.078925
36.655251	1711.079226	17.083943
35.882418	1703.005460	17.088960
35.774065	1707.051294	17.093978
36.117765	1697.273635	17.098995
36.038570	1745.315589	17.104013
36.105387	1733.780941	17.109031
36.207782	1732.020153	17.114048
36.388608	1747.361432	17.119066
36.581625	1711.166728	17.124083
35.890356	1741.166133	17.129101
36.380370	1711.766750	17.134119
36.290289	1732.214795	17.139136
36.308702	1746.257483	17.144154
36.519418	1711.412762	17.149171
36.088113	1739.413859	17.154189
36.640148	1738.511025	17.159207
36.736099	1729.370606	17.164224
36.415310	1720.958899	17.169242
36.705765	1744.095928	17.174259
36.584896	1723.017754	17.179277
36.740055	1733.161105	17.184295
36.571300	1734.426025	17.189312
36.511012	1731.777250	17.194330
36.660383	1723.748313	17.199347
36.387798	1742.721661	17.204365
36.746647	1714.892625	17.209383
36.735360	1760.465157	17.214400
36.710895	1720.682417	17.219418
36.876299	1739.796698	17.224435
36.812791	1744.475615	17.229453
37.087694	1739.742601	17.234471
37.214061	1760.447177	17.239488
36.936317	1755.394876	17.244506
37.256674	1749.147645	17.249523
36.994262	1730.662366	17.254541
37.301643	1763.672213	17.259559
37.378554	1745.415949	17.264576
37.471988	1754.785789	17.269594
37.438505	1718.869434	17.274611
36.930222	1734.910482	17.279629
37.225513	1727.454451	17.284647
37.528460	1745.138944	17.289664
37.125686	1737.254682	17.294682
37.607164	1750.186899	17.299699
37.612627	1760.583806	17.304717
37.445378	1747.318386	17.309735
37.626678	1755.821631	17.314752
37.563938	1754.436389	17.319770
37.682572	1756.240646	17.324787
37.586569	1750.146331	17.329805
37.609014	1739.710438	17.334823
37.600974	1759.542967	17.339840
37.655309	1752.224451	17.344858
37.884773	1742.861383	17.349875
37.792343	1750.947381	17.354893
37.794292	1751.971146	17.359911
37.786026	1756.225976	17.364928
37.606384	1749.492191	17.369946
38.010215	1744.137716	17.374963
37.505753	1753.160883	17.379981
37.827948	1751.479872	17.384999
37.980161	1746.495860	17.390016
37.706982	1749.219903	17.395034
37.977621	1735.030505	17.400051
38.016333	1774.652200	17.405069
38.159221	1760.527195	17.410087
38.242666	1778.908982	17.415104
38.326565	1784.357213	17.420122
38.440254	1763.038653	17.425139
38.512475	1792.302922	17.430157
38.384640	1754.833207	17.435175
38.771499	1777.648175	17.440192
38.310787	1747.321236	17.445210
38.441643	1773.472525	17.450227
38.318657	1738.452867	17.455245
38.514409	1760.576264	17.460263
38.551492	1776.948813	17.465280
38.909183	1768.027753	17.470298
38.815128	1763.877391	17.475315
38.612644	1767.255557	17.480333
38.921053	1757.074497	17.485351
38.718955	1757.419792	17.490368
38.698183	1727.961834	17.495386
38.665252	1759.791116	17.500403
38.557389	1747.170607	17.505421
38.625030	1787.048845	17.510439
38.314980	1774.605275	17.515456
38.480598	1773.804962	17.520474
38.675067	1779.501401	17.525491
38.702284	1781.430353	17.530509
38.924370	1797.944883	17.535527
39.362038	1801.338947	17.540544
39.114853	1811.211460	17.545562
39.859362	1793.027996	17.550579
39.120798	1789.339062	17.555597
38.956788	1763.814443	17.560615
38.952421	1774.409557	17.565632
38.699860	1803.450362	17.570650
39.466621	1791.962921	17.575667
39.099982	1793.001424	17.580685
39.617833	1786.351445	17.585703
39.791868	1787.497208	17.590720
39.709968	1801.669206	17.595738
39.463166	1786.467443	17.600755
39.325926	1809.784470	17.605773
39.608970	1796.398430	17.610791
39.806073	1785.860718	17.615808
39.231177	1812.190694	17.620826
39.610550	1775.319592	17.625843
39.714595	1816.376601	17.630861
39.467316	1783.527000	17.635879
39.638516	1799.988299	17.640896
39.440082	1803.353243	17.645914
40.017579	1798.183414	17.650931
39.660563	1814.032111	17.655949
40.383524	1789.312967	17.660967
40.232669	1827.132449	17.665984
39.997657	1790.392321	17.671002
40.248445	1794.039557	17.676019
40.095309	1788.777034	17.681037
39.505072	1822.428815	17.686055
39.676084	1814.682670	17.691072
40.140746	1807.795770	17.696090
40.073409	1843.992758	17.701107
40.207574	1814.920480	17.706125
39.904920	1840.252256	17.711143
40.312247	1819.814880	17.716160
40.158133	1844.202747	17.721178
40.423751	1818.032211	17.726195
40.180327	1846.697262	17.731213
40.462893	1800.972722	17.736231
40.596184	1843.031887	17.741248
40.617068	1827.614357	17.746266
40.972010	1855.933889	17.751283
40.504445	1833.528138	17.756301
41.006288	1832.771731	17.761319
40.672116	1832.373592	17.766336
40.660576	1801.174230	17.771354
40.730771	1817.590309	17.776371
40.910889	1848.710975	17.781389
40.433964	1836.814641	17.786407
41.216319	1836.007208	17.791424
41.052154	1851.128332	17.796442
41.747419	1812.048546	17.801459
41.070486	1848.452873	17.806477
40.916885	1798.582144	17.811495
41.015850	1815.495431	17.816512
40.891851	1789.355620	17.821530
41.258637	1841.369474	17.826547
41.313037	1827.831103	17.831565
41.004491	1849.840001	17.836583
41.595004	1822.511796	17.841600
41.411700	1848.260286	17.846618
41.388707	1830.738726	17.851635
41.501434	1847.623115	17.856653
41.752221	1835.354324	17.861671
41.817009	1831.796817	17.866688
41.589414	1814.429029	17.871706
41.496517	1799.949901	17.876723
41.697908	1814.761006	17.881741
41.924896	1812.834046	17.886759
41.739373	1786.833040	17.891776
41.699918	1816.299214	17.896794
42.355742	1779.421766	17.901811
41.840710	1825.255736	17.906829
41.673947	1802.673072	17.911847
41.817636	1817.957428	17.916864
41.764738	1785.737500	17.921882
41.524466	1820.645378	17.926899
41.665541	1787.228891	17.931917
41.655807	1847.594288	17.936935
41.894134	1816.240214	17.941952
41.987479	1847.794718	17.946970
42.226803	1821.054210	17.951987
42.197155	1838.110731	17.957005
42.200069	1825.425296	17.962023
41.983754	1854.650762	17.967040
41.589252	1839.110697	17.972058
42.411960	1812.689306	17.977075
42.420009	1822.842024	17.982093
42.196766	1871.137031	17.987111
41.859340	1825.453083	17.992128
41.780956	1861.239740	17.997146
42.060667	1844.338435	18.002163
42.358994	1891.085828	18.007181
41.835324	1871.625845	18.012199
42.227882	1887.046767	18.017216
42.154543	1889.469975	18.022234
41.914367	1894.839367	18.027251
43.091931	1879.430806	18.032269
42.977668	1905.893562	18.037287
43.218197	1876.105765	18.042304
42.912785	1921.527503	18.047322
43.213522	1878.897158	18.052339
43.264252	1889.291656	18.057357
42.961037	1889.744316	18.062375
43.384648	1900.983861	18.067392
43.391743	1875.840750	18.072410
43.365966	1894.380102	18.077427
43.557132	1853.654961	18.082445
43.157901	1875.889149	18.087463
43.257411	1846.666601	18.092480
42.933610	1857.490470	18.097498
43.340037	1856.801190	18.102515
43.160739	1871.578680	18.107533
43.208708	1875.132436	18.112551
43.373505	1880.484432	18.117568
43.747404	1876.418289	18.122586
43.552671	1876.614545	18.127603
43.850753	1886.997911	18.132621
43.788568	1862.723182	18.137639
43.592832	1885.258417	18.142656
43.579920	1857.362552	18.147674
44.016111	1874.039656	18.152691
43.795200	1855.111866	18.157709
43.711716	1860.659179	18.162727
43.750727	1853.292719	18.167744
43.976146	1874.568408	18.172762
43.799824	1862.790856	18.177779
43.875987	1887.313535	18.182797
43.780310	1863.571116	18.187815
43.924695	1888.828541	18.192832
44.056156	1878.554491	18.197850
44.052613	1896.473666	18.202867
44.592639	1879.524514	18.207885
43.546397	1899.849993	18.212903
44.348075	1873.466453	18.217920
43.982337	1893.939809	18.222938
43.630703	1869.775722	18.227955
44.048698	1899.326418	18.232973
43.701608	1897.668751	18.237991
44.293860	1906.913524	18.243008
44.180542	1901.326855	18.248026
44.185645	1931.863694	18.253043
44.406383	1907.570514	18.258061
44.138036	1929.897171	18.263079
44.474053	1925.670312	18.268096
45.111914	1916.029644	18.273114
44.833049	1911.424212	18.278131
44.856333	1937.685763	18.283149
44.714616	1897.968426	18.288167
45.008521	1922.031717	18.293184
44.880386	1913.173887	18.298202
44.886822	1913.523683	18.303219
45.289656	1899.915522	18.308237
44.421534	1916.119547	18.313255
44.978042	1918.289731	18.318272
44.957767	1919.919530	18.323290
44.897924	1904.341756	18.328307
45.405688	1921.583237	18.333325
45.261527	1941.906492	18.338343
45.247638	1935.084837	18.343360
45.104160	1948.247460	18.348378
44.973740	1961.223965	18.353395
45.318148	1929.588457	18.358413
44.952409	1961.081136	18.363431
45.129993	1939.714374	18.368448
45.457944	1928.115906	18.373466
45.071248	1952.169804	18.378483
45.538385	1930.539798	18.383501
45.325061	1934.405803	18.388519
45.813093	1963.176238	18.393536
46.168341	1960.435986	18.398554
46.083430	1953.446320	18.403571
46.105959	1955.132219	18.408589
45.838413	1924.800844	18.413607
45.898997	1925.165600	18.418624
45.835407	1953.231166	18.423642
45.862544	1912.418758	18.428659
46.128538	1943.258515	18.433677
45.841456	1911.907798	18.438695
46.235887	1936.755764	18.443712
46.319138	1939.518957	18.448730
46.206922	1929.810704	18.453747
46.448719	1909.132181	18.458765
46.226247	1931.755123	18.463783
46.509460	1919.359967	18.468800
46.493899	1906.498079	18.473818
46.117111	1930.232606	18.478835
46.619882	1920.753480	18.483853
46.053571	1926.682987	18.488871
46.342431	1924.102769	18.493888
45.859435	1927.497390	18.498906
46.218779	1960.192654	18.503923
46.724276	1941.685321	18.508941
46.531930	1946.831595	18.513959
46.642801	1964.084510	18.518976
46.884545	1953.286297	18.523994
46.584491	1940.362780	18.529011
46.794379	1953.335346	18.534029
46.660351	1941.156150	18.539047
46.925182	1957.838655	18.544064
46.871056	1949.519570	18.549082
47.082783	1960.931381	18.554099
47.149687	1979.890225	18.559117
47.304418	1974.781462	18.564135
47.415392	1978.406996	18.569152
47.236373	1967.034065	18.574170
47.115327	1944.981874	18.579187
47.581966	1970.658394	18.584205
47.285708	1947.083108	18.589223
47.625241	1971.832922	18.594240
47.448171	1935.460719	18.599258
46.980097	1952.983700	18.604275
47.631615	1965.535059	18.609293
47.625772	1950.197168	18.614311
47.661579	1995.451462	18.619328
47.585701	1968.650835	18.624346
47.760185	1963.007234	18.629363
47.470313	1994.667215	18.634381
47.549140	1956.369628	18.639399
47.759671	1980.617774	18.644416
47.718108	1956.937360	18.649434
47.866700	1991.749030	18.654451
47.876836	1961.997798	18.659469
47.649080	1990.174559	18.664487
47.878563	1953.863321	18.669504
48.198578	1954.299966	18.674522
47.667521	1983.964428	18.679539
48.059098	1972.728592	18.684557
48.234692	2007.046772	18.689575
48.473772	1983.140659	18.694592
48.752264	1997.502345	18.699610
48.696366	1978.395493	18.704627
48.692272	1992.250095	18.709645
48.287078	1951.235957	18.714663
48.246254	1955.829525	18.719680
48.560151	1963.087912	18.724698
48.731577	1993.922408	18.729715
48.337313	1971.866555	18.734733
48.534683	2008.709167	18.739751
48.845924	1977.124464	18.744768
48.678555	1995.862707	18.749786
48.792672	2011.875591	18.754803
48.751539	1978.969076	18.759821
48.783201	2017.033658	18.764839
48.266827	1992.603048	18.769856
49.050052	1968.503216	18.774874
48.772259	2006.352846	18.779891
49.185027	1997.308030	18.784909
49.132156	1965.040507	18.789927
48.588186	2006.913990	18.794944
48.778175	1998.601566	18.799962
49.161551	1992.448004	18.804979
49.132749	2029.042012	18.809997
49.419286	2009.171060	18.815015
49.100153	2012.899799	18.820032
49.372037	2028.701921	18.825050
49.145781	2014.184069	18.830067
49.488383	2013.471927	18.835085
49.242234	2026.644701	18.840103
49.389635	2017.948939	18.845120
49.801103	2026.797893	18.850138
49.260696	2035.100210	18.855155
49.767600	2021.827706	18.860173
49.611280	2039.744679	18.865191
49.700423	2048.281670	18.870208
50.282263	2050.073447	18.875226
50.027880	2029.178144	18.880243
50.085930	2054.205800	18.885261
50.358681	2019.707534	18.890279
50.139153	2051.332825	18.895296
50.683194	2029.562991	18.900314
50.409196	2039.612971	18.905331
50.494751	2031.540558	18.910349
50.297195	2016.401486	18.915367
50.186745	1983.189830	18.920384
50.437812	2034.211355	18.925402
50.318614	2016.703340	18.930419
50.431982	2052.223930	18.935437
50.749943	2032.511533	18.940455
50.419305	2030.396611	18.945472
50.882214	2037.245873	18.950490
50.492807	2035.989776	18.955507
50.764910	2022.070433	18.960525
50.370651	2041.637741	18.965543
50.641311	2038.478372	18.970560
51.011786	2029.833547	18.975578
50.798687	2043.144215	18.980595
50.722878	2018.684202	18.985613
50.654670	2032.923457	18.990631
50.920737	2037.947895	18.995648
50.851019	2028.755055	19.000666
51.082317	2033.794474	19.005683
51.046515	2013.630418	19.010701
51.214246	2048.846595	19.015719
51.278722	2035.968684	19.020736
51.421845	2053.353418	19.025754
51.436910	2056.552235	19.030771
51.367089	2036.491102	19.035789
51.468349	2041.368786	19.040807
51.584987	2054.790480	19.045824
51.742042	2020.445945	19.050842
51.590132	2062.297965	19.055859
51.432142	2041.099402	19.060877
51.811062	2040.485289	19.065895
51.513389	2070.479232	19.070912
51.234252	2050.342918	19.075930
51.884596	2040.210957	19.080947
51.983415	2021.840736	19.085965
51.952506	2071.425535	19.090983
51.633383	2051.858754	19.096000
52.447445	2020.259840	19.101018
51.932357	2072.245266	19.106035
52.127528	2045.064636	19.111053
52.070114	2028.251487	19.116071
51.892322	2060.326330	19.121088
52.313056	2035.551146	19.126106
52.182383	2048.900585	19.131123
52.271350	2061.379713	19.136141
52.401670	2054.072524	19.141159
52.344171	2093.729310	19.146176
52.799987	2058.670061	19.151194
52.527772	2094.181454	19.156211
52.390543	2079.493606	19.161229
52.767212	2062.696139	19.166247
52.320924	2086.374360	19.171264
52.861447	2072.398007	19.176282
52.739530	2071.254985	19.181299
52.814611	2068.030841	19.186317
53.009151	2074.878872	19.191335
52.538380	2087.883023	19.196352
52.978594	2072.791629	19.201370
53.202280	2062.424089	19.206387
52.855298	2089.962515	19.211405
53.123118	2054.368524	19.216423
52.791091	2089.867422	19.221440
52.820325	2060.573852	19.226458
52.841778	2121.458459	19.231475
53.243942	2094.204615	19.236493
53.508167	2070.184235	19.241511
53.220904	2115.020075	19.246528
53.753607	2065.130222	19.251546
53.765321	2110.149611	19.256563
53.513066	2095.818300	19.261581
54.429279	2077.262603	19.266599
53.751976	2105.558469	19.271616
53.706088	2082.303269	19.276634
54.253271	2070.491970	19.281651
54.211180	2095.375214	19.286669
54.074754	2053.746900	19.291687
54.161899	2098.386127	19.296704
53.998863	2084.828706	19.301722
54.246399	2048.125805	19.306739
53.847501	2086.956100	19.311757
53.582169	2086.314159	19.316775
54.163818	2076.172678	19.321792
54.070066	2075.221797	19.326810
54.155556	2062.351522	19.331827
54.372838	2091.086736	19.336845
54.045736	2077.475259	19.341863
54.195494	2056.641313	19.346880
54.460886	2084.745909	19.351898
54.211026	2128.024780	19.356915
54.365600	2121.941473	19.361933
54.411873	2102.351747	19.366951
54.715130	2087.783988	19.371968
54.631196	2118.499019	19.376986
54.363456	2126.403176	19.382003
54.772953	2086.821583	19.387021
55.081764	2098.134648	19.392039
54.716852	2130.785342	19.397056
54.504769	2125.399171	19.402074
54.512546	2127.391833	19.407091
55.205930	2108.413867	19.412109
55.084094	2140.214901	19.417127
55.119266	2139.893923	19.422144
55.545299	2115.680918	19.427162
55.234993	2162.353208	19.432179
55.539654	2121.165611	19.437197
55.839691	2117.605127	19.442215
55.351518	2158.186519	19.447232
55.499425	2147.508523	19.452250
55.871434	2115.737643	19.457267
55.249349	2170.592461	19.462285
55.377605	2146.820161	19.467303
55.840165	2138.303738	19.472320
55.803056	2143.389145	19.477338
55.819023	2148.897112	19.482355
55.404548	2181.923923	19.487373
56.359089	2146.961116	19.492391
56.135277	2171.591103	19.497408
56.120074	2186.354541	19.502426
56.339888	2158.590090	19.507443
55.972484	2175.413782	19.512461
56.667825	2146.134157	19.517479
56.418044	2178.264000	19.522496
56.798431	2152.176026	19.527514
56.326575	2166.805407	19.532531
56.631258	2139.060494	19.537549
56.538622	2173.159924	19.542567
56.459641	2152.275012	19.547584
56.442519	2172.395853	19.552602
56.368002	2149.646923	19.557619
56.198831	2169.876953	19.562637
56.549970	2153.807069	19.567655
56.464265	2173.731202	19.572672
56.636896	2159.890514	19.577690
56.692436	2139.733739	19.582707
56.714586	2157.918922	19.587725
57.115330	2176.929397	19.592743
56.782991	2173.690760	19.597760
57.005589	2205.403189	19.602778
57.381683	2167.449338	19.607795
57.471791	2195.354003	19.612813
57.751541	2177.219798	19.617831
57.489612	2173.859031	19.622848
57.252389	2177.161030	19.627866
57.313667	2161.783109	19.632883
57.501127	2170.794508	19.637901
57.738031	2191.856468	19.642919
57.678452	2173.418504	19.647936
57.363902	2175.072449	19.652954
57.264729	2184.780034	19.657971
57.697510	2178.523345	19.662989
57.792172	2167.683933	19.668007
57.934823	2188.245735	19.673024
57.913680	2161.789964	19.678042
57.696973	2181.775112	19.683059
57.560626	2158.392638	19.688077
57.785219	2210.356560	19.693095
57.724535	2187.469292	19.698112
57.761581	2191.659607	19.703130
57.898928	2205.559500	19.708147
57.842154	2197.569469	19.713165
58.229199	2212.843750	19.718183
58.434928	2241.947633	19.723200
58.432407	2210.549317	19.728218
58.562588	2237.757091	19.733235
58.862668	2220.668838	19.738253
58.944814	2226.343253	19.743271
59.054073	2201.961962	19.748288
58.748472	2237.820388	19.753306
59.278039	2206.187788	19.758323
58.643230	2208.032025	19.763341
59.020360	2174.639140	19.768359
59.145404	2237.803624	19.773376
59.157375	2235.892809	19.778394
59.240610	2204.396670	19.783411
59.398143	2213.436465	19.788429
59.351607	2221.779683	19.793447
59.242210	2183.283415	19.798464
58.947843	2225.393797	19.803482
59.519041	2190.703596	19.808499
59.282104	2229.086070	19.813517
59.620026	2209.783185	19.818535
59.213805	2207.015662	19.823552
59.754161	2223.956570	19.828570
59.500465	2193.417134	19.833587
59.595184	2230.263309	19.838605
59.437043	2192.128734	19.843623
59.605277	2219.250965	19.848640
59.706282	2191.452699	19.853658
59.766849	2202.877009	19.858675
59.647082	2232.761902	19.863693
59.806948	2217.444496	19.868711
60.114686	2248.775342	19.873728
60.284786	2235.101733	19.878746
60.329567	2256.971528	19.883763
60.262265	2252.682260	19.888781
60.159466	2249.508466	19.893799
60.543043	2211.254420	19.898816
60.550131	2263.286251	19.903834
60.461734	2240.739959	19.908851
60.579521	2258.558433	19.913869
60.948936	2223.390652	19.918887
60.673870	2265.647515	19.923904
60.397125	2228.382012	19.928922
60.916140	2238.470057	19.933939
60.578113	2272.007932	19.938957
60.585282	2235.726723	19.943975
61.075560	2231.785863	19.948992
60.395814	2261.281895	19.954010
60.515126	2240.042753	19.959027
60.519743	2261.522542	19.964045
60.868553	2288.196092	19.969063
60.786338	2266.081375	19.974080
61.153386	2278.596573	19.979098
61.196110	2283.984703	19.984115
61.168573	2305.187314	19.989133
61.710261	2288.276754	19.994151
61.709830	2306.380777	19.999168
61.793665	2273.978291	20.004186
62.136603	2303.428521	20.009203
61.959431	2263.501896	20.014221
62.051119	2275.546602	20.019239
61.645101	2266.334090	20.024256
61.957280	2245.622630	20.029274
62.361548	2274.016918	20.034291
61.852824	2262.408455	20.039309
62.314778	2229.123047	20.044327
62.140136	2214.759576	20.049344
61.933366	2257.649703	20.054362
61.975253	2285.129632	20.059379
62.076936	2271.005984	20.064397
62.417811	2302.358405	20.069415
62.210582	2276.125591	20.074432
62.303502	2307.125076	20.079450
62.428110	2261.941823	20.084467
62.581230	2291.147007	20.089485
62.435887	2293.635249	20.094503
62.519635	2269.939061	20.099520
62.652230	2273.898649	20.104538
62.625904	2309.190451	20.109555
62.992270	2294.573882	20.114573
63.055421	2308.208842	20.119591
63.141615	2311.429407	20.124608
62.655764	2295.783074	20.129626
62.733126	2318.509821	20.134643
62.992190	2323.157934	20.139661
63.293431	2301.876319	20.144679
63.483894	2324.725045	20.149696
63.165252	2295.808958	20.154714
63.268060	2330.202434	20.159731
63.246738	2300.341476	20.164749
63.097373	2326.072027	20.169767
63.338149	2320.459404	20.174784
63.437423	2328.359416	20.179802
63.906511	2346.743350	20.184819
63.908199	2335.913919	20.189837
63.934144	2344.678251	20.194855
64.192749	2345.127064	20.199872
63.810324	2333.231764	20.204890
64.040250	2352.633882	20.209907
64.161595	2340.568575	20.214925
64.057286	2342.127662	20.219943
64.120640	2323.609339	20.224960
64.262002	2357.159844	20.229978
64.662031	2322.168636	20.234995
64.599245	2308.584007	20.240013
64.429670	2353.909139	20.245031
64.828282	2316.165251	20.250048
64.730283	2347.359655	20.255066
64.958159	2312.301537	20.260083
64.594768	2356.080557	20.265101
64.462394	2322.992748	20.270119
64.764677	2294.011470	20.275136
64.621390	2352.176699	20.280154
64.907017	2359.457099	20.285171
64.656904	2357.770540	20.290189
64.537964	2327.601035	20.295207
64.910046	2312.904881	20.300224
65.042011	2359.470308	20.305242
65.464212	2346.010450	20.310259
65.136338	2369.047299	20.315277
64.858502	2344.443553	20.320295
65.454242	2333.852103	20.325312
65.146314	2378.114724	20.330330
65.415777	2342.517407	20.335347
65.579233	2347.493821	20.340365
65.255031	2373.542572	20.345383
65.820137	2356.697416	20.350400
65.916656	2349.176022	20.355418
66.115996	2395.328894	20.360435
65.797450	2389.531717	20.365453
66.008567	2365.167732	20.370471
65.864661	2391.196416	20.375488
66.084753	2420.605909	20.380506
65.920412	2385.727356	20.385523
66.360617	2371.940544	20.390541
66.037885	2396.983106	20.395559
66.332544	2352.610131	20.400576
66.125279	2380.318743	20.405594
66.206556	2388.541783	20.410611
65.975048	2364.787169	20.415629
66.307455	2391.837136	20.420647
66.820732	2410.655360	20.425664
66.534563	2393.772081	20.430682
66.895225	2397.613534	20.435699
66.900940	2406.407085	20.440717
66.956096	2399.086540	20.445735
67.074653	2410.847848	20.450752
66.891562	2379.877529	20.455770
66.902220	2416.704546	20.460787
67.031269	2407.670114	20.465805
67.262770	2402.647280	20.470823
67.176342	2389.358156	20.475840
67.183761	2374.746047	20.480858
67.483631	2410.677457	20.485875
67.241868	2406.131231	20.490893
67.546455	2405.517162	20.495911
67.588905	2429.696905	20.500928
67.798164	2402.028059	20.505946
67.685463	2432.222924	20.510963
67.451939	2416.416666	20.515981
68.245809	2392.284553	20.520999
68.111011	2429.009735	20.526016
67.386845	2446.132100	20.531034
67.502252	2429.594536	20.536051
68.259008	2411.472856	20.541069
67.874010	2412.031382	20.546087
68.064570	2461.691527	20.551104
67.764426	2450.054371	20.556122
68.021664	2442.785740	20.561139
68.810326	2422.875055	20.566157
68.744229	2433.904445	20.571175
68.645713	2448.729416	20.576192
68.919247	2417.997675	20.581210
68.996013	2451.432851	20.586227
68.767793	2427.587942	20.591245
68.881918	2454.642159	20.596263
69.012547	2446.890321	20.601280
68.815712	2431.840366	20.606298
69.254009	2406.260256	20.611315
68.923043	2438.868472	20.616333
68.620671	2477.151129	20.621351
69.254942	2457.203666	20.626368
69.196184	2449.763613	20.631386
69.042622	2472.043693	20.636403
69.509237	2442.755902	20.641421
69.287568	2472.681135	20.646439
69.504488	2465.257679	20.651456
69.728016	2462.522610	20.656474
69.596236	2448.122971	20.661491
69.746286	2469.746627	20.666509
69.278460	2456.149366	20.671527
69.910624	2476.147427	20.676544
69.936828	2464.922286	20.681562
69.632559	2493.827200	20.686579
70.191447	2477.856761	20.691597
70.081404	2488.095632	20.696615
70.393597	2488.217350	20.701632
70.079364	2467.293989	20.706650
70.305495	2487.565250	20.711667
70.635725	2468.934183	20.716685
70.488161	2491.923596	20.721703
70.811464	2454.388785	20.726720
70.761795	2496.873872	20.731738
70.705026	2475.391889	20.736755
71.133353	2461.252938	20.741773
70.842517	2471.024311	20.746791
70.922451	2481.288729	20.751808
70.747335	2479.874928	20.756826
70.774742	2460.701457	20.761843
71.125634	2467.114161	20.766861
70.613462	2480.277065	20.771879
71.474872	2478.788432	20.776896
71.412198	2498.102903	20.781914
71.530053	2507.260113	20.786931
71.685832	2503.056327	20.791949
71.466034	2500.741964	20.796967
71.709303	2513.424977	20.801984
71.843815	2496.118971	20.807002
71.767275	2493.569394	20.812019
71.818048	2507.591928	20.817037
71.737176	2493.229746	20.822055
71.863962	2509.680845	20.827072
72.164334	2486.070105	20.832090
72.076867	2496.399769	20.837107
72.268937	2504.584758	20.842125
71.959549	2498.362908	20.847143
72.102047	2489.783271	20.852160
71.977294	2490.457610	20.857178
71.940929	2502.985420	20.862195
72.556770	2502.411383	20.867213
72.142652	2506.647775	20.872231
72.454060	2516.541020	20.877248
72.760399	2515.740254	20.882266
72.630115	2503.970569	20.887283
73.041679	2527.488326	20.892301
72.846344	2519.954392	20.897319
73.205968	2495.995181	20.902336
72.943991	2530.635288	20.907354
73.128731	2502.152928	20.912371
72.954515	2516.522037	20.917389
72.654259	2525.860769	20.922407
73.079275	2514.296700	20.927424
73.512994	2545.898340	20.932442
73.201710	2535.194963	20.937459
73.265879	2559.547648	20.942477
73.108129	2548.966079	20.947495
73.309726	2540.268443	20.952512
73.351147	2539.063154	20.957530
73.381391	2549.891641	20.962547
73.677260	2562.508891	20.967565
73.306212	2576.206261	20.972583
74.039876	2573.523542	20.977600
73.855720	2579.673955	20.982618
73.623265	2579.382272	20.987635
74.040476	2574.748217	20.992653
74.201682	2605.201014	20.997671
74.193201	2606.104586	21.002688
74.131053	2605.021206	21.007706
74.107108	2602.405018	21.012723
74.502739	2590.044854	21.017741
74.271048	2613.093493	21.022759
74.150419	2603.842335	21.027776
74.881665	2619.530166	21.032794
74.854714	2622.693334	21.037811
75.343437	2617.515358	21.042829
75.139152	2635.788373	21.047847
75.414942	2599.207003	21.052864
75.389247	2621.291518	21.057882
75.237853	2624.352612	21.062899
75.798038	2596.652609	21.067917
75.377744	2605.330156	21.072935
75.932619	2590.577047	21.077952
75.280029	2605.763466	21.082970
75.760251	2588.966975	21.087987
75.461149	2600.223207	21.093005
75.843951	2590.158705	21.098023
75.656514	2623.327287	21.103040
75.612092	2596.610938	21.108058
75.584239	2635.440157	21.113075
75.967327	2589.416309	21.118093
75.873364	2630.411235	21.123111
76.153456	2598.340125	21.128128
75.815286	2609.988009	21.133146
76.084784	2639.293320	21.138163
76.121172	2640.814271	21.143181
76.551743	2641.676150	21.148199
76.345413	2628.743363	21.153216
76.339954	2656.919001	21.158234
76.626977	2636.397415	21.163251
76.363529	2646.306119	21.168269
76.709238	2633.643973	21.173287
76.745835	2670.375468	21.178304
76.988746	2661.565772	21.183322
77.011762	2657.621442	21.188339
77.066245	2673.377920	21.193357
77.087287	2651.598532	21.198375
77.292398	2658.412120	21.203392
77.181305	2667.783703	21.208410
77.103871	2650.656825	21.213427
77.687143	2651.691783	21.218445
77.185311	2674.874051	21.223463
77.758166	2635.340433	21.228480
77.761240	2657.936402	21.233498
77.592536	2667.619212	21.238515
77.473353	2635.346616	21.243533
77.656811	2693.343120	21.248551
78.100373	2675.754010	21.253568
77.998505	2677.273414	21.258586
77.744112	2695.507299	21.263603
78.407172	2679.785103	21.268621
78.196697	2684.153465	21.273639
78.003947	2676.366550	21.278656
78.227064	2688.975060	21.283674
78.172033	2686.906544	21.288691
78.588281	2672.728415	21.293709
78.444694	2722.755788	21.298727
78.729093	2697.642548	21.303744
79.125636	2692.498123	21.308762
78.831805	2711.681412	21.313779
79.024784	2705.029343	21.318797
78.921463	2705.072593	21.323815
79.039817	2701.234180	21.328832
78.816299	2693.511941	21.333850
79.012136	2700.905153	21.338867
79.257800	2709.982333	21.343885
79.069371	2732.396580	21.348903
79.353996	2715.518655	21.353920
79.538739	2740.947320	21.358938
79.576861	2714.116126	21.363955
79.872461	2730.837093	21.368973
79.738788	2713.164578	21.373991
79.906956	2736.756882	21.379008
80.125631	2715.675035	21.384026
80.075991	2691.960101	21.389043
80.006562	2715.380244	21.394061
80.246607	2750.123304	21.399079
79.982821	2713.980856	21.404096
80.276069	2753.867463	21.409114
80.095720	2766.488464	21.414131
80.418448	2748.234219	21.419149
80.579688	2730.871759	21.424167
80.078091	2780.633925	21.429184
80.508296	2747.768496	21.434202
80.636008	2759.154220	21.439219
81.206675	2769.510490	21.444237
80.689221	2768.564985	21.449255
81.160652	2777.371021	21.454272
81.721075	2762.823724	21.459290
81.176013	2780.429186	21.464307
81.276500	2797.540019	21.469325
81.488256	2768.568303	21.474343
81.560557	2794.082636	21.479360
81.588085	2784.529291	21.484378
81.794574	2769.664015	21.489395
81.977776	2782.732038	21.494413
82.319900	2735.097071	21.499431
81.634145	2752.706843	21.504448
81.590424	2740.849225	21.509466
81.559359	2746.567067	21.514483
82.130754	2784.004075	21.519501
82.197122	2758.478723	21.524519
81.983035	2787.911786	21.529536
81.911236	2759.792326	21.534554
81.806774	2756.661159	21.539571
82.117160	2798.766433	21.544589
82.111179	2787.304697	21.549607
82.038615	2779.946908	21.554624
82.187345	2804.817455	21.559642
82.480012	2808.842122	21.564659
82.589515	2782.891393	21.569677
82.833207	2829.268250	21.574695
82.584431	2830.403649	21.579712
83.100364	2804.868670	21.584730
83.060311	2846.257546	21.589747
83.214613	2813.683735	21.594765
83.228379	2832.332817	21.599783
83.261980	2839.304409	21.604800
83.562348	2823.088506	21.609818
83.338958	2822.511418	21.614835
83.330670	2825.570971	21.619853
83.689730	2829.460779	21.624871
83.629564	2867.019944	21.629888
84.300328	2843.344060	21.634906
84.038516	2843.400784	21.639923
84.299525	2859.868633	21.644941
84.389498	2839.009280	21.649959
84.235330	2867.083972	21.654976
84.471054	2829.981406	21.659994
84.165677	2870.316173	21.665011
84.456874	2826.345038	21.670029
84.291756	2871.009558	21.675047
84.165595	2859.099703	21.680064
84.477866	2830.976283	21.685082
84.499230	2869.966606	21.690099
84.778862	2859.444852	21.695117
85.179621	2863.866825	21.700135
85.083579	2898.203682	21.705152
85.307130	2857.494954	21.710170
85.306863	2880.254622	21.715187
85.211857	2897.093912	21.720205
85.476342	2862.970954	21.725223
85.797026	2852.733692	21.730240
85.483937	2886.372829	21.735258
85.366924	2854.474598	21.740275
85.694255	2877.045160	21.745293
85.589102	2855.354022	21.750311
85.436961	2874.229403	21.755328
85.482842	2854.021266	21.760346
85.515270	2895.848646	21.765363
86.080742	2881.031418	21.770381
85.831025	2894.609055	21.775399
86.123520	2885.429494	21.780416
86.160270	2898.657051	21.785434
86.364671	2901.667761	21.790451
86.336275	2889.864211	21.795469
86.676384	2900.429601	21.800487
86.385037	2876.619976	21.805504
86.691798	2909.534213	21.810522
86.552634	2903.845088	21.815539
86.705405	2905.450550	21.820557
86.878362	2934.052917	21.825575
86.819174	2903.971797	21.830592
87.116852	2926.146794	21.835610
86.816875	2928.888695	21.840627
87.182579	2903.125008	21.845645
87.425856	2953.821431	21.850663
87.231744	2949.302830	21.855680
87.607007	2918.858222	21.860698
87.168566	2967.224213	21.865715
87.403614	2938.504085	21.870733
87.764701	2909.936964	21.875751
87.513119	2966.765065	21.880768
87.677728	2963.912661	21.885786
88.165400	2962.851704	21.890803
88.117728	2985.153437	21.895821
88.092061	2971.666100	21.900839
87.892020	2981.028469	21.905856
88.388996	2952.393975	21.910874
88.267091	2992.835116	21.915891
87.930569	2966.410080	21.920909
88.888738	2964.284580	21.925927
88.670942	3015.248236	21.930944
88.601302	2976.500475	21.935962
88.847679	3006.577131	21.940979
88.996804	2975.731123	21.945997
89.082762	2976.885523	21.951015
89.386757	2983.372797	21.956032
89.329112	2971.779143	21.961050
89.459158	2983.319627	21.966067
89.371298	2983.202309	21.971085
89.550039	2989.570332	21.976103
89.599774	2991.701153	21.981120
90.135750	3006.899041	21.986138
90.082885	3019.916821	21.991155
90.399964	3018.835081	21.996173
90.111074	2981.488564	22.001191
90.024919	2998.390273	22.006208
90.189856	2990.144996	22.011226
90.154562	2994.918137	22.016243
90.317358	3007.068526	22.021261
90.445442	3005.655881	22.026279
90.472893	2994.994900	22.031296
90.537244	3003.161207	22.036314
90.388760	3026.288474	22.041331
90.662691	2986.444463	22.046349
90.653776	3021.081563	22.051367
90.659716	2990.333081	22.056384
90.934641	3011.466468	22.061402
90.922998	3003.681961	22.066419
91.005957	3026.534775	22.071437
91.342216	3030.699646	22.076455
91.106571	3044.994118	22.081472
91.050743	3040.447932	22.086490
91.252391	3043.966460	22.091507
91.728979	3027.863817	22.096525
91.537905	3024.857311	22.101543
91.433207	3037.999000	22.106560
91.854316	3042.248668	22.111578
92.085029	3053.187150	22.116595
91.838976	3062.420828	22.121613
92.200451	3055.337428	22.126631
92.407293	3062.015637	22.131648
92.157389	3056.254439	22.136666
92.521105	3059.253938	22.141683
92.509553	3052.556453	22.146701
92.499288	3045.134321	22.151719
92.161415	3068.520749	22.156736
92.708224	3053.843976	22.161754
92.817936	3058.217241	22.166771
92.653942	3076.662937	22.171789
92.937094	3077.986482	22.176807
93.017180	3072.114452	22.181824
93.224403	3058.614283	22.186842
92.985040	3073.635395	22.191859
92.941780	3088.027447	22.196877
93.613563	3080.031668	22.201895
93.419774	3120.340679	22.206912
93.636782	3076.087224	22.211930
93.726516	3104.605660	22.216947
93.753456	3103.296445	22.221965
94.174670	3091.470596	22.226983
93.986938	3093.196447	22.232000
94.121236	3094.625534	22.237018
94.067446	3107.817377	22.242035
94.039444	3080.712093	22.247053
94.736575	3099.254126	22.252071
94.311797	3124.435338	22.257088
94.864350	3114.547138	22.262106
94.761323	3104.324562	22.267123
94.528154	3127.109166	22.272141
94.764357	3128.513355	22.277159
94.513713	3131.218322	22.282176
94.723394	3112.771629	22.287194
94.809938	3114.269687	22.292211
94.698102	3145.573408	22.297229
95.264763	3148.618439	22.302247
95.173832	3133.543790	22.307264
95.278365	3162.920510	22.312282
95.723183	3145.969351	22.317299
95.544017	3140.837912	22.322317
95.543931	3159.650873	22.327335
95.633016	3156.074224	22.332352
95.930634	3153.867605	22.337370
95.918299	3181.436531	22.342387
96.272953	3162.651235	22.347405
96.374924	3167.731341	22.352423
96.216541	3175.216674	22.357440
96.585951	3176.958315	22.362458
96.522272	3164.699225	22.367475
96.332035	3165.315602	22.372493
96.378531	3169.908214	22.377511
96.297908	3183.323076	22.382528
96.615180	3184.421732	22.387546
96.797292	3193.049191	22.392563
96.671350	3208.966378	22.397581
96.892991	3212.835727	22.402599
96.878886	3194.077726	22.407616
96.839620	3214.669202	22.412634
97.226591	3210.632866	22.417651
97.230283	3220.045494	22.422669
97.426598	3251.260976	22.427687
97.575851	3226.361882	22.432704
97.700899	3234.459646	22.437722
98.063434	3227.019667	22.442739
98.159600	3245.798513	22.447757
98.585802	3233.786904	22.452775
98.519615	3238.805749	22.457792
98.580690	3211.509035	22.462810
98.880960	3226.124114	22.467827
98.388045	3202.593087	22.472845
98.531596	3209.613399	22.477863
98.577845	3229.284315	22.482880
98.758877	3239.552027	22.487898
98.937326	3240.256713	22.492915
99.184992	3253.709752	22.497933
99.524563	3225.932830	22.502951
99.305462	3242.094594	22.507968
99.294617	3238.000547	22.512986
99.490894	3231.298159	22.518003
99.226339	3231.786374	22.523021
99.636600	3225.555651	22.528039
99.529040	3238.123761	22.533056
99.768241	3242.349793	22.538074
99.802969	3226.792492	22.543091
99.499092	3231.723379	22.548109
99.834644	3235.767287	22.553127
100.101929	3258.706704	22.558144
99.649958	3272.376722	22.563162
100.256102	3263.416717	22.568179
100.149823	3251.987127	22.573197
100.347482	3265.247569	22.578215
100.145712	3274.751202	22.583232
100.343167	3289.544778	22.588250
100.497674	3277.517461	22.593267
100.204602	3289.354554	22.598285
100.941852	3265.540749	22.603303
100.958046	3291.543151	22.608320
101.377573	3282.309263	22.613338
101.479049	3291.820404	22.618355
101.385418	3288.182398	22.623373
101.806301	3290.373647	22.628391
101.652384	3300.885166	22.633408
101.518110	3319.618258	22.638426
102.432922	3298.794275	22.643443
101.786066	3298.965095	22.648461
101.837838	3293.116369	22.653479
101.968451	3311.169282	22.658496
102.227918	3293.273697	22.663514
102.247601	3279.682877	22.668531
101.910667	3307.735642	22.673549
102.249112	3284.126197	22.678567
101.959342	3292.178439	22.683584
102.476615	3316.189552	22.688602
102.720929	3326.155406	22.693619
102.557761	3332.303573	22.698637
102.767876	3320.570196	22.703655
102.876652	3333.726095	22.708672
102.890694	3307.852583	22.713690
103.243763	3331.930808	22.718707
103.187132	3346.971046	22.723725
103.541150	3330.403856	22.728743
103.110254	3363.586979	22.733760
103.459804	3343.985772	22.738778
103.658429	3349.664080	22.743795
103.508382	3331.028264	22.748813
103.639037	3382.102039	22.753831
104.359823	3342.829250	22.758848
104.136991	3398.940212	22.763866
104.283018	3382.613791	22.768883
104.323204	3358.787484	22.773901
104.840717	3370.196487	22.778919
104.721504	3357.527617	22.783936
104.623158	3379.410121	22.788954
104.993048	3347.376539	22.793971
104.552113	3378.608951	22.798989
104.923815	3353.632480	22.804007
105.127586	3393.176417	22.809024
104.876711	3376.597073	22.814042
105.404390	3409.365518	22.819059
105.159736	3385.809554	22.824077
105.402187	3403.506509	22.829095
105.654141	3371.273003	22.834112
105.519655	3397.673256	22.839130
105.898864	3388.282904	22.844147
105.793208	3391.832425	22.849165
106.089264	3387.126978	22.854183
106.158314	3421.268835	22.859200
106.393082	3394.246142	22.864218
106.239721	3430.865106	22.869235
105.870784	3420.395234	22.874253
106.408260	3390.538909	22.879271
106.517091	3415.870733	22.884288
106.105592	3413.522283	22.889306
106.721078	3418.635443	22.894323
106.803841	3406.268633	22.899341
106.968080	3432.194978	22.904359
106.976879	3437.546468	22.909376
106.969391	3424.689031	22.914394
107.525231	3433.182316	22.919411
107.122545	3419.927731	22.924429
106.850304	3439.390133	22.929447
107.230273	3441.108100	22.934464
107.557882	3444.965335	22.939482
107.496859	3445.827779	22.944499
107.704404	3462.506995	22.949517
107.988118	3456.902828	22.954535
108.025623	3448.167104	22.959552
108.019804	3479.342937	22.964570
108.252570	3467.612910	22.969587
108.349541	3481.508665	22.974605
108.231531	3489.067954	22.979623
108.516537	3475.381159	22.984640
108.364545	3475.613090	22.989658
109.012611	3485.293640	22.994675
108.731809	3494.439523	22.999693
109.010874	3506.911607	23.004711
109.203112	3494.096205	23.009728
108.947804	3497.700290	23.014746
109.090402	3515.984382	23.019763
109.432845	3496.147335	23.024781
109.535109	3526.532011	23.029799
109.883172	3521.463468	23.034816
109.483332	3518.589258	23.039834
109.830808	3537.691824	23.044851
109.953590	3517.383194	23.049869
109.919606	3526.289157	23.054887
110.251195	3543.732939	23.059904
110.668983	3553.107288	23.064922
110.891783	3545.454233	23.069939
110.582180	3543.091874	23.074957
110.867634	3565.494768	23.079975
111.016835	3551.722576	23.084992
110.970351	3542.808253	23.090010
110.894585	3551.302415	23.095027
111.191700	3546.235695	23.100045
111.078993	3524.926272	23.105063
111.065697	3549.051472	23.110080
111.106024	3547.069888	23.115098
111.380554	3557.842869	23.120115
111.394120	3580.479498	23.125133
111.861223	3577.633022	23.130151
111.794492	3565.086181	23.135168
111.684287	3596.350489	23.140186
111.824254	3568.387639	23.145203
111.922282	3596.616240	23.150221
112.270498	3595.000105	23.155239
112.422496	3603.950403	23.160256
112.415291	3611.494448	23.165274
112.664617	3589.388574	23.170291
112.339703	3608.993324	23.175309
112.708568	3583.445045	23.180327
112.786218	3621.719662	23.185344
112.534093	3607.010830	23.190362
113.304464	3615.218300	23.195379
113.116824	3646.170975	23.200397
113.004306	3614.769867	23.205415
113.464937	3614.385740	23.210432
113.313105	3654.803593	23.215450
113.613859	3646.682604	23.220467
114.071983	3648.876626	23.225485
113.722770	3680.784132	23.230503
114.332696	3647.810943	23.235520
113.928109	3680.292856	23.240538
114.121786	3643.251570	23.245555
114.210994	3666.465448	23.250573
113.888117	3675.625231	23.255591
114.873431	3646.141423	23.260608
114.574790	3688.425823	23.265626
114.694423	3674.120182	23.270643
114.729701	3688.368149	23.275661
114.214279	3692.716993	23.280679
115.282374	3672.605110	23.285696
115.248108	3726.052084	23.290714
115.344130	3694.829155	23.295731
115.240150	3710.531785	23.300749
115.254592	3718.362697	23.305767
115.435565	3712.825946	23.310784
115.985883	3706.459417	23.315802
116.607159	3745.759965	23.320819
116.372960	3743.091353	23.325837
116.118238	3710.248019	23.330855
116.459772	3746.957990	23.335872
116.293950	3739.946539	23.340890
116.704671	3698.788717	23.345907
116.524099	3731.279863	23.350925
116.259589	3714.493066	23.355943
116.515010	3749.333599	23.360960
116.544516	3733.115828	23.365978
116.953238	3757.483227	23.370995
116.991081	3731.083639	23.376013
117.213635	3777.739057	23.381031
117.971567	3779.101818	23.386048
117.370210	3776.389478	23.391066
117.835516	3782.427402	23.396083
117.813916	3784.822220	23.401101
118.113410	3763.919489	23.406119
118.006908	3796.921289	23.411136
118.063230	3762.130116	23.416154
118.159571	3783.119255	23.421171
118.401740	3759.618792	23.426189
118.091934	3791.848279	23.431207
118.478115	3770.724047	23.436224
118.513768	3795.435751	23.441242
118.505291	3795.102818	23.446259
118.770128	3797.304083	23.451277
118.760980	3799.213143	23.456295
119.022602	3807.512066	23.461312
118.622193	3787.075665	23.466330
119.303044	3830.488863	23.471347
119.123780	3818.102914	23.476365
119.334236	3816.920914	23.481383
119.728371	3825.415829	23.486400
119.923611	3803.173517	23.491418
119.899271	3862.413701	23.496435
119.964907	3846.598305	23.501453
120.091053	3859.194976	23.506471
120.213143	3836.272043	23.511488
120.012652	3870.752125	23.516506
120.350687	3840.479093	23.521523
120.260939	3872.602088	23.526541
120.525749	3871.173855	23.531559
120.972634	3867.148244	23.536576
120.471070	3895.805767	23.541594
120.534786	3893.928962	23.546611
121.239983	3879.638313	23.551629
121.078291	3921.504301	23.556647
120.882527	3903.478391	23.561664
121.690259	3887.017587	23.566682
121.978556	3939.463659	23.571699
122.180463	3908.350828	23.576717
122.461930	3952.767307	23.581735
122.764228	3914.152841	23.586752
122.680576	3889.243343	23.591770
122.453752	3909.695789	23.596787
122.552628	3880.282838	23.601805
122.234296	3902.133547	23.606823
122.589847	3901.701666	23.611840
122.701442	3920.417563	23.616858
122.810243	3921.309595	23.621875
123.081958	3910.650693	23.626893
122.915176	3917.334591	23.631911
123.382342	3927.936325	23.636928
123.504784	3949.826170	23.641946
123.633215	3957.740512	23.646963
123.765305	3950.307808	23.651981
123.699936	3947.941052	23.656999
123.470264	3959.226583	23.662016
123.652456	3944.507160	23.667034
123.817588	3971.567073	23.672051
124.134411	3946.488217	23.677069
124.142270	3988.804851	23.682087
124.188995	3993.068086	23.687104
124.443169	3963.649086	23.692122
124.078439	3985.939967	23.697139
124.730056	3976.879462	23.702157
124.680656	4009.138704	23.707175
124.912285	4001.625600	23.712192
124.676601	4040.398866	23.717210
124.687608	4005.643446	23.722227
125.241092	4014.146891	23.727245
125.092116	4069.827794	23.732263
125.305127	4019.445768	23.737280
125.639089	4059.090318	23.742298
126.034189	4055.124046	23.747315
126.614452	4069.630828	23.752333
126.351709	4057.485324	23.757351
126.640577	4056.389921	23.762368
126.490098	4072.679319	23.767386
126.746005	4060.248167	23.772403
126.893055	4082.849343	23.777421
125.999360	4056.095816	23.782439
126.156083	4071.392265	23.787456
126.592449	4069.855637	23.792474
126.574024	4094.397899	23.797491
127.310923	4095.850580	23.802509
126.894604	4105.607642	23.807527
127.510988	4099.705547	23.812544
127.483503	4112.241186	23.817562
127.427320	4126.589907	23.822579
127.889977	4117.087459	23.827597
127.612603	4124.656751	23.832615
127.971316	4148.869155	23.837632
128.576710	4131.440515	23.842650
128.293079	4149.712333	23.847667
128.539447	4145.611635	23.852685
128.691991	4139.058191	23.857703
128.801669	4158.237244	23.862720
129.277693	4144.421042	23.867738
129.071374	4169.329284	23.872755
129.486459	4163.285410	23.877773
129.380484	4173.417039	23.882791
129.674246	4164.915358	23.887808
129.637979	4179.725863	23.892826
129.665777	4161.195935	23.897843
129.561461	4157.782822	23.902861
129.677185	4169.028391	23.907879
130.167682	4185.986633	23.912896
129.989163	4192.056581	23.917914
130.293034	4200.105132	23.922931
130.675694	4190.496608	23.927949
130.506159	4213.592918	23.932967
130.504256	4192.268790	23.937984
130.816632	4181.304283	23.943002
130.428361	4223.304801	23.948019
130.688366	4215.706826	23.953037
130.942369	4224.557071	23.958055
130.831524	4218.780316	23.963072
131.202437	4229.423577	23.968090
131.097571	4253.803678	23.973107
131.771848	4236.201097	23.978125
131.415785	4230.623911	23.983143
131.890242	4240.030577	23.988160
131.660866	4239.816238	23.993178
131.928511	4256.187066	23.998195
132.416983	4266.422218	24.003213
132.011939	4265.198294	24.008231
132.289066	4267.203369	24.013248
132.189521	4276.168225	24.018266
132.219940	4299.013313	24.023283
132.894176	4296.187960	24.028301
132.836645	4301.546408	24.033319
132.816613	4315.043110	24.038336
133.309184	4316.622089	24.043354
133.253775	4318.765149	24.048371
133.609977	4324.745964	24.053389
133.551844	4332.242647	24.058407
133.917392	4343.673502	24.063424
134.022484	4340.394517	24.068442
133.675448	4345.641021	24.073459
134.320448	4343.002825	24.078477
134.217817	4340.708025	24.083495
134.094450	4348.997053	24.088512
134.665001	4368.471058	24.093530
134.799563	4372.015553	24.098547
134.863933	4378.963308	24.103565
135.180751	4374.765569	24.108583
134.984941	4373.934644	24.113600
135.470873	4379.455843	24.118618
135.141514	4408.162425	24.123635
135.829478	4409.073068	24.128653
135.962299	4395.648041	24.133671
135.685666	4394.713574	24.138688
135.848777	4401.576372	24.143706
136.041618	4409.966058	24.148723
136.238645	4412.015392	24.153741
135.924267	4430.276726	24.158759
136.698729	4417.792490	24.163776
136.852322	4435.401812	24.168794
137.078212	4428.035726	24.173811
137.185417	4405.627181	24.178829
137.208347	4433.693944	24.183847
137.711869	4422.381760	24.188864
137.982383	4408.687756	24.193882
137.276446	4422.117701	24.198899
137.660889	4420.868583	24.203917
137.761119	4434.766297	24.208935
138.166677	4418.686838	24.213952
138.451121	4442.717267	24.218970
138.345929	4438.169862	24.223987
138.383062	4425.106981	24.229005
138.526015	4433.102652	24.234023
138.495951	4437.286219	24.239040
138.654168	4414.801087	24.244058
138.739864	4426.208186	24.249075
138.532373	4423.457309	24.254093
138.747279	4451.122981	24.259111
138.875020	4463.782852	24.264128
138.952466	4466.854253	24.269146
139.061112	4479.032596	24.274163
139.409150	4479.023552	24.279181
139.375202	4491.543239	24.284199
139.495356	4486.284935	24.289216
139.456307	4502.857549	24.294234
139.478244	4531.203136	24.299251
139.878568	4512.032027	24.304269
139.836859	4531.407984	24.309287
140.436521	4552.161432	24.314304
140.434706	4545.409792	24.319322
140.559380	4549.238321	24.324339
140.950585	4556.142705	24.329357
140.868570	4585.112277	24.334375
141.202512	4569.698580	24.339392
141.165452	4585.706930	24.344410
141.061793	4587.413253	24.349427
141.226993	4584.993113	24.354445
141.719181	4605.585985	24.359463
142.029995	4588.449216	24.364480
142.390079	4608.195457	24.369498
142.024393	4595.092021	24.374515
142.721807	4629.540074	24.379533
143.244221	4604.343934	24.384551
143.098625	4618.109520	24.389568
143.128657	4626.839957	24.394586
143.168804	4620.243646	24.399603
143.736362	4596.512969	24.404621
143.284210	4616.359611	24.409639
143.556612	4618.205796	24.414656
143.829118	4607.639880	24.419674
143.579723	4634.048090	24.424691
143.356990	4634.768036	24.429709
143.752077	4602.711971	24.434727
143.751847	4627.877627	24.439744
143.677857	4632.427762	24.444762
143.990327	4620.142882	24.449779
143.950658	4659.714108	24.454797
144.210579	4652.283484	24.459815
144.140925	4689.485393	24.464832
144.644319	4663.701391	24.469850
144.822891	4690.054057	24.474867
144.820048	4721.630114	24.479885
144.987117	4700.450591	24.484903
145.229728	4719.252035	24.489920
145.268633	4742.728948	24.494938
145.735055	4722.714723	24.499955
145.988128	4693.797126	24.504973
145.840349	4703.513340	24.509991
145.978164	4763.430662	24.515008
146.448137	4746.621553	24.520026
146.515610	4766.036267	24.525043
146.565932	4782.020672	24.530061
146.623467	4757.659892	24.535079
147.062482	4737.506055	24.540096
147.086073	4770.704065	24.545114
147.075038	4744.828081	24.550131
147.125764	4781.037910	24.555149
147.538141	4763.249109	24.560167
147.057717	4801.397870	24.565184
147.675289	4770.554431	24.570202
147.824463	4782.622724	24.575219
147.846470	4807.189626	24.580237
148.548771	4786.480044	24.585255
148.277938	4804.907968	24.590272
148.730592	4798.417308	24.595290
148.489406	4805.019067	24.600307
148.620406	4801.726409	24.605325
148.618285	4785.632093	24.610343
148.658620	4833.909805	24.615360
149.005283	4824.992597	24.620378
149.155718	4822.895739	24.625395
149.790401	4828.653003	24.630413
150.120650	4816.417833	24.635431
150.192209	4812.484851	24.640448
150.349632	4830.445684	24.645466
150.527201	4819.108857	24.650483
150.548525	4812.842720	24.655501
151.043092	4831.111677	24.660519
150.510944	4836.070044	24.665536
150.568845	4808.705568	24.670554
150.729858	4845.742869	24.675571
150.585856	4847.275504	24.680589
150.837816	4834.767235	24.685607
151.027965	4876.688412	24.690624
151.329875	4857.139990	24.695642
150.999578	4874.953642	24.700659
151.703733	4874.747797	24.705677
151.610968	4874.643828	24.710695
151.492685	4911.978349	24.715712
152.025488	4896.834696	24.720730
152.162376	4907.914614	24.725747
152.171666	4938.268266	24.730765
152.589214	4912.669014	24.735783
152.654128	4944.547063	24.740800
152.721755	4918.382892	24.745818
152.673757	4960.765514	24.750835
153.189516	4959.195691	24.755853
153.462531	4958.921697	24.760871
153.558611	4969.319814	24.765888
153.464693	4946.445323	24.770906
153.682417	4984.591816	24.775923
153.907100	4966.842922	24.780941
154.537854	4989.619335	24.785959
154.518030	4973.379739	24.790976
154.644163	4970.114567	24.795994
154.666327	4979.739361	24.801011
154.481604	4976.772341	24.806029
155.055331	4965.833244	24.811047
154.794233	4982.975175	24.816064
155.162157	4984.769992	24.821082
155.306468	5002.995094	24.826099
155.403684	5011.674927	24.831117
155.447652	4995.617088	24.836135
155.393700	5007.797407	24.841152
155.802696	5012.331233	24.846170
156.197791	5026.897602	24.851187
155.909406	5040.026311	24.856205
156.549224	5029.472338	24.861223
156.163774	5035.219249	24.866240
156.388828	5032.849284	24.871258
156.621158	5034.164601	24.876275
156.680599	5062.081206	24.881293
156.818502	5039.761205	24.886311
156.689623	5060.047013	24.891328
157.261040	5079.589487	24.896346
157.573895	5061.865756	24.901363
157.058425	5096.675056	24.906381
157.727922	5099.999922	24.911399
157.580595	5099.204491	24.916416
157.707720	5133.666769	24.921434
158.048951	5126.886919	24.926451
157.907337	5157.887359	24.931469
158.676005	5153.154001	24.936487
158.990273	5160.263682	24.941504
159.169913	5166.644318	24.946522
159.365955	5173.915246	24.951539
159.323805	5163.307841	24.956557
159.497959	5151.033558	24.961575
159.685850	5168.205608	24.966592
159.757399	5182.682108	24.971610
159.825838	5176.129813	24.976627
160.004770	5184.810882	24.981645
160.101529	5190.511658	24.986663
160.445735	5206.202648	24.991680
160.613653	5214.411109	24.996698
160.857606	5211.610923	25.001715
160.757226	5208.325169	25.006733
161.091310	5207.483664	25.011751
160.973015	5219.082028	25.016768
161.356691	5219.103496	25.021786
161.443543	5236.138326	25.026803
161.635222	5231.638537	25.031821
161.849441	5215.053761	25.036839
161.887237	5254.930492	25.041856
162.263507	5244.111568	25.046874
162.295468	5248.700071	25.051891
162.173753	5258.125347	25.056909
162.442063	5246.620319	25.061927
162.694143	5276.868306	25.066944
162.883215	5286.127620	25.071962
162.626865	5264.181669	25.076979
162.534471	5300.278706	25.081997
163.339833	5292.701804	25.087015
163.462733	5296.799865	25.092032
163.819214	5317.197459	25.097050
164.413713	5306.718959	25.102067
163.971613	5317.357316	25.107085
164.434802	5308.470805	25.112103
164.433856	5306.529394	25.117120
164.621386	5305.870950	25.122138
164.843936	5315.898280	25.127155
165.085634	5330.011875	25.132173
165.089463	5329.416544	25.137191
165.071297	5346.211778	25.142208
165.524553	5331.540589	25.147226
165.537039	5315.377281	25.152243
165.239016	5338.174861	25.157261
165.718174	5348.005535	25.162279
165.769410	5355.265024	25.167296
165.781284	5355.964908	25.172314
166.060263	5372.437451	25.177331
166.028792	5386.099022	25.182349
166.059697	5393.515179	25.187367
166.545099	5414.729417	25.192384
166.547102	5424.257016	25.197402
166.995454	5424.379889	25.202419
166.925007	5433.350250	25.207437
167.327155	5437.282679	25.212455
167.540761	5446.157414	25.217472
167.465142	5458.059914	25.222490
168.214112	5470.999240	25.227507
168.199775	5468.508454	25.232525
168.375670	5463.420288	25.237543
168.241072	5477.645151	25.242560
168.740576	5470.150750	25.247578
168.852835	5481.799103	25.252595
168.949045	5487.116165	25.257613
169.331206	5504.178178	25.262631
169.658416	5508.880970	25.267648
169.448419	5495.139837	25.272666
169.707344	5499.101410	25.277683
169.705979	5517.410165	25.282701
170.170841	5502.342025	25.287719
170.146781	5518.258843	25.292736
170.531681	5509.111702	25.297754
170.542112	5513.225395	25.302771
170.693988	5523.694469	25.307789
170.907368	5519.435017	25.312807
171.083244	5532.769434	25.317824
171.024980	5539.214908	25.322842
171.331509	5534.803713	25.327859
171.227263	5534.910049	25.332877
171.437463	5563.667389	25.337895
171.741306	5562.099824	25.342912
171.688023	5559.772576	25.347930
171.808439	5570.098795	25.352947
172.249199	5578.074363	25.357965
172.268674	5579.518072	25.362983
172.466697	5603.435158	25.368000
172.641742	5602.095817	25.373018
172.817969	5598.965706	25.378035
172.967364	5609.520989	25.383053
173.273456	5604.551269	25.388071
173.330024	5640.514463	25.393088
173.804764	5620.307314	25.398106
173.855009	5615.587646	25.403123
173.751441	5640.408040	25.408141
174.234785	5650.074613	25.413159
174.327703	5646.900342	25.418176
174.090654	5647.163167	25.423194
174.474797	5656.344415	25.428211
174.609599	5687.785739	25.433229
174.802403	5675.481300	25.438247
174.691947	5683.766658	25.443264
175.197946	5693.439875	25.448282
175.432857	5708.059208	25.453299
175.144179	5726.473817	25.458317
175.641482	5714.997219	25.463335
175.910253	5723.676873	25.468352
175.952141	5747.556932	25.473370
176.434958	5738.419217	25.478387
176.342848	5750.782459	25.483405
176.416269	5779.602149	25.488423
176.565395	5761.148420	25.493440
176.800220	5791.840000	25.498458
177.429726	5788.484176	25.503475
177.068535	5794.160637	25.508493
177.468787	5791.207190	25.513511
177.846438	5809.012167	25.518528
178.096770	5823.568578	25.523546
177.946480	5814.966809	25.528563
178.423435	5817.173910	25.533581
178.780325	5814.948807	25.538599
178.845170	5848.183579	25.543616
179.064291	5836.471944	25.548634
179.296178	5827.486681	25.553651
179.199374	5842.053606	25.558669
179.522744	5845.257601	25.563687
179.523287	5838.607267	25.568704
179.395441	5851.168254	25.573722
179.702584	5869.150545	25.578739
180.064373	5858.280774	25.583757
180.129915	5880.653824	25.588775
180.735146	5883.452568	25.593792
180.624334	5883.688192	25.598810
180.831479	5870.510386	25.603827
180.723910	5882.995787	25.608845
180.898267	5885.168530	25.613863
181.029775	5904.448660	25.618880
181.428358	5900.364914	25.623898
181.514014	5899.618050	25.628915
181.954438	5905.702532	25.633933
182.089401	5923.427539	25.638951
182.417912	5922.531029	25.643968
182.213978	5937.576156	25.648986
182.430629	5932.067507	25.654003
182.291077	5939.065031	25.659021
182.558004	5962.819876	25.664039
183.299216	5954.544804	25.669056
182.885881	5965.641641	25.674074
182.946149	5964.129387	25.679092
183.098134	5985.492013	25.684109
183.458074	5986.020789	25.689127
184.031730	5998.675410	25.694144
183.951871	6009.632577	25.699162
184.296826	6018.157073	25.704180
184.714464	6025.677115	25.709197
184.451736	6032.941357	25.714215
184.778981	6026.614136	25.719232
185.037772	6061.479291	25.724250
185.076274	6041.453618	25.729268
184.948280	6045.647745	25.734285
185.209655	6083.954559	25.739303
185.606162	6090.390716	25.744320
185.602685	6095.961487	25.749338
185.993161	6104.181386	25.754356
186.409561	6113.585149	25.759373
186.247142	6118.442508	25.764391
186.974035	6122.086545	25.769408
186.825425	6123.183396	25.774426
187.148625	6130.351133	25.779444
187.218946	6140.585821	25.784461
187.683103	6156.106077	25.789479
187.728355	6150.375270	25.794496
187.441480	6157.434146	25.799514
188.020228	6162.402312	25.804532
188.404478	6178.840883	25.809549
188.076338	6188.341355	25.814567
188.593966	6193.963628	25.819584
188.696845	6186.746095	25.824602
188.783647	6201.436735	25.829620
188.957037	6214.899622	25.834637
189.072521	6211.880558	25.839655
189.309901	6226.477984	25.844672
189.513028	6241.477411	25.849690
189.634646	6248.783554	25.854708
189.957913	6269.349050	25.859725
190.074825	6266.619275	25.864743
190.658759	6261.295850	25.869760
190.561835	6266.223853	25.874778
190.951799	6291.183022	25.879796
190.958730	6304.281507	25.884813
191.087948	6306.204238	25.889831
191.185629	6297.057557	25.894848
191.557533	6312.598979	25.899866
191.780306	6308.872803	25.904884
192.110725	6316.157495	25.909901
191.669121	6330.806616	25.914919
191.951468	6323.871179	25.919936
192.024964	6344.013193	25.924954
192.718386	6344.469942	25.929972
192.627307	6363.837294	25.934989
193.045326	6358.559167	25.940007
193.377351	6369.546139	25.945024
193.487636	6382.994063	25.950042
193.577837	6354.529543	25.955060
193.601414	6386.547902	25.960077
193.694586	6379.330250	25.965095
194.010096	6417.795308	25.970112
194.540290	6393.378511	25.975130
194.583121	6441.592638	25.980148
194.809004	6425.804791	25.985165
194.672644	6450.016519	25.990183
195.225244	6433.344968	25.995200
195.298166	6450.681607	26.000218
195.228878	6456.646948	26.005236
195.473345	6474.012129	26.010253
195.901083	6476.093430	26.015271
196.412968	6476.976442	26.020288
196.263677	6487.672807	26.025306
196.575183	6504.012403	26.030324
196.541170	6484.732535	26.035341
197.000548	6527.164656	26.040359
197.228008	6506.540969	26.045376
197.248802	6529.289556	26.050394
197.381959	6528.933983	26.055412
197.730488	6527.193190	26.060429
197.492841	6560.178023	26.065447
197.747007	6532.199214	26.070464
198.168475	6542.566243	26.075482
198.405388	6579.967947	26.080500
198.115280	6567.366819	26.085517
198.855846	6574.919065	26.090535
199.549003	6595.452803	26.095552
199.618477	6595.945297	26.100570
199.277814	6613.342548	26.105588
199.841520	6609.302314	26.110605
199.321734	6618.522833	26.115623
199.948050	6641.012990	26.120640
200.174739	6628.923445	26.125658
200.570546	6667.146613	26.130676
200.616361	6663.022123	26.135693
200.616384	6648.575311	26.140711
200.896016	6671.533839	26.145728
201.011843	6682.726240	26.150746
200.760210	6686.619250	26.155764
201.193434	6704.938876	26.160781
201.452271	6726.298915	26.165799
201.744746	6711.408098	26.170816
201.826087	6756.459754	26.175834
202.365049	6743.330563	26.180852
202.385443	6742.162904	26.185869
202.604966	6765.461608	26.190887
203.136711	6766.949660	26.195904
203.044495	6765.957306	26.200922
202.996431	6783.904497	26.205940
203.336279	6784.305118	26.210957
203.540997	6800.607777	26.215975
203.905008	6797.508065	26.220992
203.466738	6827.892098	26.226010
204.311655	6820.854952	26.231028
204.598960	6830.974490	26.236045
204.358109	6829.556569	26.241063
204.978578	6862.169247	26.246080
204.969236	6876.627258	26.251098
205.377382	6863.070344	26.256116
205.594330	6875.563072	26.261133
205.795504	6889.884469	26.266151
205.836838	6891.325608	26.271168
205.938206	6906.039017	26.276186
206.050456	6900.584420	26.281204
206.121507	6928.123468	26.286221
206.341428	6920.173301	26.291239
206.708338	6924.955985	26.296256
207.142380	6961.687566	26.301274
207.235361	6975.621093	26.306292
207.947955	6980.263717	26.311309
207.947315	6976.631213	26.316327
208.230211	6979.954425	26.321344
208.547120	7001.642354	26.326362
208.499734	7021.012253	26.331380
209.053502	6981.813092	26.336397
208.589100	7011.296848	26.341415
208.967210	7032.229969	26.346432
209.413706	7020.673137	26.351450
209.212555	7033.892771	26.356468
209.603467	7044.014823	26.361485
210.065847	7057.447361	26.366503
209.894083	7060.476417	26.371520
210.054029	7067.375588	26.376538
210.179398	7088.650421	26.381556
210.723855	7095.452119	26.386573
210.958663	7107.876892	26.391591
211.183811	7110.413095	26.396608
211.367262	7122.170203	26.401626
211.285748	7138.064875	26.406644
211.726443	7143.894122	26.411661
211.814779	7144.022484	26.416679
211.973460	7152.842488	26.421696
212.089269	7184.925762	26.426714
212.623300	7171.972440	26.431732
212.816009	7167.253174	26.436749
212.712567	7224.953727	26.441767
213.401820	7203.692895	26.446784
213.172862	7192.813249	26.451802
213.413052	7227.748637	26.456820
214.072829	7222.947821	26.461837
214.019867	7221.332320	26.466855
214.149944	7228.120666	26.471872
214.360791	7242.523478	26.476890
214.188170	7250.520630	26.481908
214.658604	7264.039409	26.486925
214.970333	7273.979899	26.491943
215.463358	7283.931625	26.496960
215.362709	7276.081151	26.501978
215.284885	7294.965288	26.506996
215.922250	7316.778058	26.512013
216.130179	7320.889884	26.517031
216.005378	7309.162674	26.522048
216.530887	7325.089823	26.527066
216.830164	7344.092519	26.532084
217.016692	7342.615077	26.537101
216.993118	7365.146989	26.542119
217.543454	7369.216051	26.547136
217.492467	7363.379734	26.552154
217.618853	7397.841117	26.557172
217.813040	7405.609929	26.562189
217.908511	7415.782479	26.567207
218.553018	7421.888570	26.572224
218.839160	7433.819180	26.577242
218.826897	7445.344156	26.582260
219.221905	7444.399984	26.587277
219.284263	7449.558705	26.592295
219.484714	7458.878159	26.597312
219.839253	7491.046785	26.602330
219.976427	7485.864177	26.607348
220.041424	7487.026215	26.612365
220.665165	7513.573403	26.617383
221.039008	7504.234824	26.622400
221.261014	7510.331978	26.627418
221.068469	7522.750472	26.632436
221.518537	7524.240611	26.637453
221.657417	7547.136382	26.642471
221.933357	7532.838288	26.647488
222.035918	7540.858612	26.652506
222.427654	7569.416242	26.657524
222.465986	7572.961118	26.662541
222.616815	7550.772971	26.667559
222.623289	7592.776771	26.672576
223.027798	7579.907477	26.677594
223.340896	7611.107303	26.682612
224.045537	7591.142526	26.687629
223.858215	7645.924785	26.692647
224.399864	7612.918265	26.697664
224.217991	7614.065373	26.702682
224.160008	7639.673396	26.707700
224.741310	7653.287378	26.712717
224.989599	7646.553467	26.717735
225.304077	7648.687617	26.722752
225.391793	7671.847457	26.727770
225.082852	7664.382479	26.732788
225.528432	7691.090574	26.737805
225.651256	7673.320062	26.742823
225.565229	7703.398730	26.747840
226.214706	7716.750117	26.752858
226.276284	7724.323069	26.757876
226.488805	7723.954820	26.762893
226.467476	7757.802459	26.767911
227.175719	7763.066848	26.772928
227.070877	7760.328872	26.777946
226.886395	7799.764769	26.782964
227.588676	7805.480983	26.787981
227.915248	7831.000499	26.792999
228.071711	7838.305808	26.798016
228.164649	7832.706024	26.803034
228.272970	7860.216860	26.808052
228.694325	7892.985511	26.813069
228.861783	7888.539144	26.818087
229.048825	7903.480660	26.823104
229.911514	7921.283266	26.828122
229.843787	7930.989616	26.833140
230.160356	7932.426328	26.838157
230.609693	7944.885279	26.843175
230.671765	7943.127042	26.848192
230.990284	7979.634064	26.853210
230.927533	7964.629447	26.858228
231.484137	7993.636085	26.863245
231.560765	7986.994692	26.868263
231.641292	8010.015358	26.873280
232.219436	8005.163576	26.878298
232.179289	8024.593428	26.883316
232.504325	8037.741094	26.888333
232.573864	8030.804169	26.893351
232.923412	8044.835503	26.898368
233.293964	8067.519680	26.903386
233.397009	8057.649518	26.908404
233.707215	8085.913479	26.913421
233.995683	8095.599355	26.918439
234.037067	8098.205151	26.923456
234.399198	8104.216480	26.928474
234.478448	8123.042795	26.933492
234.914948	8123.084199	26.938509
235.215068	8131.064696	26.943527
235.189156	8137.511647	26.948544
235.710774	8148.416221	26.953562
235.538493	8170.575691	26.958580
235.538253	8188.414661	26.963597
236.187088	8181.965245	26.968615
236.270379	8208.160757	26.973632
237.125605	8200.549291	26.978650
236.554281	8243.475586	26.983668
237.185350	8224.701991	26.988685
237.283448	8250.544276	26.993703
237.744391	8223.377574	26.998720
237.836361	8267.091302	27.003738
237.950888	8254.548563	27.008756
238.047911	8274.660333	27.013773
238.254141	8276.494724	27.018791
238.429626	8313.874392	27.023808
238.746248	8293.184452	27.028826
238.456604	8347.199516	27.033844
238.909786	8333.025060	27.038861
239.155931	8374.964536	27.043879
239.611247	8360.013074	27.048896
239.999307	8402.811301	27.053914
240.464558	8388.757621	27.058932
240.602337	8418.263052	27.063949
240.814516	8430.716148	27.068967
240.760475	8418.451152	27.073984
241.459929	8439.607301	27.079002
241.516297	8450.179441	27.084020
241.734462	8464.603518	27.089037
242.344073	8459.981854	27.094055
241.931657	8489.026669	27.099072
242.566338	8490.578765	27.104090
242.710966	8508.483944	27.109108
242.664067	8523.423240	27.114125
243.359655	8516.106175	27.119143
243.446652	8572.269212	27.124160
243.735562	8561.693950	27.129178
243.774019	8565.058846	27.134196
243.927943	8594.641527	27.139213
244.130415	8603.411348	27.144231
244.421819	8611.139331	27.149248
244.340928	8628.514831	27.154266
244.998516	8630.949323	27.159284
244.993080	8652.982193	27.164301
245.486915	8671.698268	27.169319
245.400230	8673.318151	27.174336
246.259410	8690.473459	27.179354
246.739079	8712.259915	27.184372
246.741804	8705.981329	27.189389
247.409956	8728.002160	27.194407
247.374212	8723.583608	27.199424
247.794576	8749.365949	27.204442
247.877091	8737.499518	27.209460
248.180201	8754.490154	27.214477
248.640276	8747.096025	27.219495
248.269605	8791.369751	27.224512
248.782394	8760.532799	27.229530
249.007802	8808.164050	27.234548
249.219328	8787.280078	27.239565
249.589625	8823.918624	27.244583
249.168315	8819.793238	27.249600
249.909601	8814.437162	27.254618
250.117264	8831.303818	27.259636
250.130115	8889.416411	27.264653
250.541678	8856.175294	27.269671
250.424861	8885.044316	27.274688
250.776149	8919.822361	27.279706
250.803351	8923.071491	27.284724
251.147940	8925.066866	27.289741
251.443091	8947.996540	27.294759
251.929411	8942.561842	27.299776
252.065486	8966.085040	27.304794
252.492012	8956.795396	27.309812
252.873133	8989.315165	27.314829
253.328124	8955.302431	27.319847
252.975984	9010.733682	27.324864
253.410772	9014.691394	27.329882
254.028184	9006.918742	27.334900
253.878913	9037.115621	27.339917
254.132647	9054.110140	27.344935
254.540304	9055.019387	27.349952
254.918212	9054.389466	27.354970
254.464764	9097.704675	27.359988
255.173156	9083.351522	27.365005
255.624905	9122.959806	27.370023
255.326811	9113.668310	27.375040
256.226250	9147.212205	27.380058
255.899341	9147.228930	27.385076
256.207420	9150.586003	27.390093
256.635962	9175.066227	27.395111
257.118514	9203.586553	27.400128
257.367404	9192.355432	27.405146
257.281783	9240.193835	27.410164
257.578991	9226.907040	27.415181
257.848317	9255.864744	27.420199
258.048924	9276.081752	27.425216
257.934327	9290.538419	27.430234
258.748219	9290.567687	27.435252
258.342377	9353.738664	27.440269
258.960161	9328.265178	27.445287
259.057062	9379.258813	27.450304
259.417416	9375.802690	27.455322
259.650173	9414.785242	27.460340
260.020324	9423.476885	27.465357
260.192975	9444.346608	27.470375
260.825159	9432.644229	27.475392
261.064222	9489.065041	27.480410
261.425945	9470.049533	27.485428
261.483884	9518.740219	27.490445
261.942912	9522.820115	27.495463
262.538206	9516.724530	27.500480
262.510624	9552.685416	27.505498
263.016001	9546.657662	27.510516
262.989787	9567.050500	27.515533
263.845487	9563.896262	27.520551
263.188676	9607.361423	27.525568
263.732705	9590.620065	27.530586
264.234598	9600.920162	27.535604
264.068484	9636.990678	27.540621
264.471288	9621.992038	27.545639
264.758149	9667.344739	27.550656
265.266546	9643.258608	27.555674
265.376526	9656.042612	27.560692
265.581903	9688.682017	27.565709
266.072507	9674.384658	27.570727
265.710623	9708.953593	27.575744
266.202060	9699.528026	27.580762
266.235108	9734.410232	27.585780
266.691791	9715.077881	27.590797
266.748960	9763.714400	27.595815
266.903290	9759.604026	27.600832
267.218036	9800.748051	27.605850
267.751446	9809.936432	27.610868
267.863566	9819.480773	27.615885
268.310273	9847.169943	27.620903
268.527572	9851.938083	27.625920
268.438569	9874.222545	27.630938
269.097783	9864.567496	27.635956
269.252286	9931.357727	27.640973
269.549996	9921.030361	27.645991
269.991254	9912.817088	27.651008
270.543489	9952.391092	27.656026
270.926082	9957.002681	27.661044
270.920051	9956.628297	27.666061
271.371417	9980.955503	27.671079
271.503265	9992.513774	27.676096
271.468693	9999.804949	27.681114
272.065253	9985.724135	27.686132
272.080513	10047.561555	27.691149
272.463428	10030.835945	27.696167
272.888433	10059.533125	27.701184
273.162240	10071.938815	27.706202
273.492373	10072.617316	27.711220
273.556450	10129.198667	27.716237
274.240199	10109.399548	27.721255
274.326180	10093.532157	27.726272
274.292305	10142.707742	27.731290
274.637121	10121.143561	27.736308
274.941890	10165.166129	27.741325
275.250570	10161.548476	27.746343
275.362864	10202.740429	27.751360
275.898504	10185.289908	27.756378
275.861114	10233.656563	27.761396
275.986234	10243.147162	27.766413
276.573694	10215.892956	27.771431
276.585471	10274.422669	27.776448
277.117963	10301.011808	27.781466
277.609129	10283.474219	27.786484
277.430148	10327.975717	27.791501
277.891771	10339.252688	27.796519
278.042271	10327.469391	27.801536
277.996511	10366.432699	27.806554
278.900592	10377.239006	27.811572
278.554623	10403.592945	27.816589
279.451081	10389.147598	27.821607
279.554466	10432.802474	27.826624
280.088781	10424.747624	27.831642
280.376769	10424.279151	27.836660
280.612900	10464.348348	27.841677
280.699932	10471.433463	27.846695
281.102607	10460.388588	27.851712
281.523636	10491.473745	27.856730
281.816157	10497.639588	27.861748
281.856095	10493.871876	27.866765
282.438013	10509.410985	27.871783
282.263901	10545.300405	27.876800
282.773750	10527.705254	27.881818
283.117827	10534.288260	27.886836
282.869290	10561.468625	27.891853
283.221159	10580.785798	27.896871
283.173467	10594.454725	27.901888
283.683777	10599.479003	27.906906
283.903079	10614.749806	27.911924
284.145932	10661.821863	27.916941
285.128269	10636.336475	27.921959
285.836871	10655.049933	27.926976
285.916320	10662.585324	27.931994
286.164638	10680.524975	27.937012
286.359518	10680.042216	27.942029
286.255972	10686.308641	27.947047
286.648867	10726.918614	27.952064
287.117318	10715.630121	27.957082
287.523334	10714.277138	27.962100
287.381164	10763.112353	27.967117
287.869201	10739.331897	27.972135
288.136987	10758.456507	27.977152
288.267467	10777.022614	27.982170
288.459726	10797.694347	27.987188
288.897318	10815.993165	27.992205
288.980888	10807.473218	27.997223
288.890803	10855.921099	28.002240
289.479456	10860.076332	28.007258
289.829313	10883.699109	28.012276
289.970641	10917.735335	28.017293
290.310766	10915.611736	28.022311
290.794037	10945.696683	28.027328
290.965194	10960.308130	28.032346
291.159674	10973.940773	28.037364
291.720228	11008.416831	28.042381
291.640831	11009.990941	28.047399
291.932966	11053.590778	28.052416
292.523645	11041.200425	28.057434
292.914248	11091.449081	28.062452
293.164385	11085.793521	28.067469
293.566220	11090.805350	28.072487
293.960648	11120.538058	28.077504
293.994657	11109.807246	28.082522
294.615300	11147.746154	28.087540
294.787404	11127.799213	28.092557
294.895394	11171.862581	28.097575
295.112240	11172.477737	28.102592
295.562179	11177.013260	28.107610
295.855103	11199.797989	28.112628
296.238568	11195.840776	28.117645
296.449626	11238.360508	28.122663
296.711812	11212.005939	28.127680
296.906415	11262.278924	28.132698
297.333955	11247.994858	28.137716
297.307395	11283.633101	28.142733
297.849944	11269.348788	28.147751
297.824865	11328.511789	28.152768
297.896359	11329.705755	28.157786
298.515540	11320.803845	28.162804
298.476520	11390.044799	28.167821
298.929153	11392.971274	28.172839
299.632653	11397.442844	28.177856
299.656012	11445.801345	28.182874
300.002994	11439.462425	28.187892
300.454293	11453.008533	28.192909
300.846088	11496.581963	28.197927
300.831615	11489.362089	28.202944
301.402277	11496.317094	28.207962
301.836995	11532.539585	28.212980
302.101359	11540.941593	28.217997
302.255462	11558.100826	28.223015
302.640249	11576.713571	28.228032
302.619382	11575.499381	28.233050
303.103989	11623.268251	28.238068
303.467903	11599.878892	28.243085
303.625828	11650.520265	28.248103
303.974472	11639.225785	28.253120
304.290456	11661.462905	28.258138
304.873127	11691.971100	28.263156
304.935140	11694.038258	28.268173
305.358995	11720.965586	28.273191
305.650050	11723.301227	28.278208
306.196794	11745.666190	28.283226
306.300260	11751.194871	28.288244
306.659825	11778.589822	28.293261
307.068321	11771.117451	28.298279
307.341595	11821.262095	28.303296
307.249436	11828.660137	28.308314
307.930475	11809.553420	28.313332
307.939555	11824.324939	28.318349
308.141810	11888.807029	28.323367
309.083139	11869.275067	28.328384
309.187079	11872.863632	28.333402
309.418471	11937.382606	28.338420
309.621199	11910.335818	28.343437
310.050219	11965.052916	28.348455
310.232044	11945.134242	28.353472
310.516937	11991.185492	28.358490
310.962493	11977.899602	28.363508
311.161344	11997.228813	28.368525
311.498065	12028.575751	28.373543
311.959120	12029.855660	28.378560
312.215027	12046.195634	28.383578
312.546050	12051.814879	28.388596
313.106208	12061.265435	28.393613
313.130930	12080.566227	28.398631
313.371891	12079.053885	28.403648
313.605255	12075.553254	28.408666
313.981206	12107.605806	28.413684
314.204350	12106.091972	28.418701
314.168931	12125.695588	28.423719
314.632193	12156.784145	28.428736
314.961514	12171.127964	28.433754
315.194319	12172.160522	28.438772
315.225009	12213.103365	28.443789
315.757067	12211.145773	28.448807
315.907817	12257.956502	28.453824
316.045529	12237.384514	28.458842
316.298410	12302.505894	28.463860
316.711226	12304.490275	28.468877
316.878988	12359.893672	28.473895
317.713975	12360.438709	28.478912
317.751458	12377.589712	28.483930
317.949350	12409.435352	28.488948
318.609810	12441.232531	28.493965
319.075203	12456.844375	28.498983
319.728412	12461.587371	28.504000
319.646695	12498.562712	28.509018
321.178715	12480.143232	28.514036
321.170854	12493.584388	28.519053
321.821349	12473.000022	28.524071
322.115484	12516.137415	28.529088
322.529133	12525.479382	28.534106
322.717421	12515.430383	28.539124
322.811596	12538.740344	28.544141
323.054130	12527.507767	28.549159
323.288410	12541.056777	28.554176
323.314672	12575.211885	28.559194
323.521950	12574.440989	28.564212
324.191992	12583.170313	28.569229
323.910620	12592.482976	28.574247
324.349079	12608.428471	28.579264
324.361293	12618.456072	28.584282
324.501730	12669.865153	28.589300
324.773200	12666.345722	28.594317
325.039869	12726.562342	28.599335
325.738851	12740.554010	28.604352
325.504127	12756.507566	28.609370
326.430953	12795.962254	28.614388
326.527964	12806.388120	28.619405
326.690544	12821.798103	28.624423
326.960595	12891.625952	28.629440
326.981791	12889.271521	28.634458
327.752461	12891.628127	28.639476
327.759921	12967.775343	28.644493
328.165601	12968.353600	28.649511
328.926091	13015.604145	28.654528
328.769875	13007.109368	28.659546
329.194073	13050.828120	28.664564
329.944360	13043.582060	28.669581
330.149972	13100.585283	28.674599
330.924578	13082.277915	28.679616
331.454508	13095.916873	28.684634
332.089505	13112.393976	28.689652
332.148906	13123.347912	28.694669
332.520764	13143.278154	28.699687
333.006979	13145.832636	28.704704
332.851340	13162.233888	28.709722
333.110367	13169.002610	28.714740
333.815672	13188.210330	28.719757
333.917100	13225.095480	28.724775
334.169355	13221.260003	28.729792
334.564819	13234.892572	28.734810
334.687308	13254.597240	28.739828
335.197792	13282.995310	28.744845
335.208129	13278.683785	28.749863
335.714313	13311.144557	28.754880
335.726892	13351.308194	28.759898
336.288843	13354.514391	28.764916
336.915371	13362.993124	28.769933
336.830995	13403.984667	28.774951
337.330701	13418.038239	28.779968
337.781444	13421.581158	28.784986
338.095842	13463.539281	28.790004
338.384151	13465.237664	28.795021
338.345320	13496.143322	28.800039
339.004539	13515.252931	28.805056
339.101563	13530.585723	28.810074
339.457028	13563.109227	28.815092
340.073638	13586.638429	28.820109
340.127025	13603.028689	28.825127
340.969322	13629.553773	28.830144
340.926281	13665.610337	28.835162
341.233378	13646.217626	28.840180
341.646021	13711.191084	28.845197
341.863621	13712.012170	28.850215
342.414183	13741.107634	28.855232
342.782981	13759.585013	28.860250
343.190049	13772.862589	28.865268
343.868186	13801.403857	28.870285
343.781381	13812.926493	28.875303
344.363069	13834.158039	28.880320
344.380308	13863.583527	28.885338
344.954201	13879.442856	28.890356
344.959080	13891.995599	28.895373
345.329875	13935.691657	28.900391
345.751608	13930.446057	28.905408
346.158728	13985.399549	28.910426
346.502602	13977.821186	28.915444
347.071573	14013.428523	28.920461
347.226316	14016.202266	28.925479
347.350244	14054.617167	28.930496
347.988791	14048.649586	28.935514
348.050358	14090.708664	28.940532
348.769356	14112.621463	28.945549
348.699476	14110.772550	28.950567
349.724125	14154.499948	28.955584
349.716386	14141.977225	28.960602
350.088410	14192.427060	28.965620
350.710830	14160.581445	28.970637
350.871972	14196.633786	28.975655
350.783761	14220.102020	28.980672
351.161222	14214.440765	28.985690
351.381181	14250.996509	28.990708
352.126490	14289.546484	28.995725
352.182117	14270.631316	29.000743
352.697101	14338.972659	29.005760
352.464172	14354.590779	29.010778
353.301694	14345.508088	29.015796
353.841157	14412.368713	29.020813
353.687383	14405.038190	29.025831
354.475720	14443.482514	29.030848
354.544033	14447.089175	29.035866
354.879470	14485.476182	29.040884
355.340877	14502.420630	29.045901
355.825216	14532.502799	29.050919
356.114351	14569.841870	29.055936
356.683766	14566.786012	29.060954
356.525039	14611.151886	29.065972
357.586190	14604.583628	29.070989
357.851674	14664.258437	29.076007
358.220319	14670.759545	29.081024
358.492692	14686.850395	29.086042
358.648672	14702.503429	29.091060
359.579901	14690.235753	29.096077
359.382023	14768.134663	29.101095
360.008308	14745.232998	29.106112
360.243128	14797.357849	29.111130
360.817896	14793.585527	29.116148
361.188039	14848.166492	29.121165
360.851080	14843.360394	29.126183
361.734010	14860.098149	29.131200
361.643027	14909.856405	29.136218
362.438149	14907.403634	29.141236
362.957978	14966.014440	29.146253
363.032983	14961.945914	29.151271
363.610437	14999.550747	29.156288
364.072430	14998.467070	29.161306
364.190066	15048.901128	29.166324
364.303744	15043.942668	29.171341
364.913676	15072.864426	29.176359
365.473846	15125.621367	29.181376
365.945161	15131.296066	29.186394
366.036321	15119.941750	29.191412
366.697165	15157.682470	29.196429
367.260884	15160.872841	29.201447
367.295054	15210.084099	29.206464
367.609484	15200.544620	29.211482
367.615580	15195.295744	29.216500
367.866395	15256.360910	29.221517
368.012537	15253.786742	29.226535
369.020696	15250.299214	29.231552
368.911990	15321.993412	29.236570
369.224576	15315.254437	29.241588
369.637077	15359.722065	29.246605
369.771435	15354.133770	29.251623
370.397236	15404.482910	29.256640
371.071073	15409.066712	29.261658
371.361835	15436.629780	29.266676
372.007562	15432.243273	29.271693
372.464084	15472.647486	29.276711
372.510959	15508.751629	29.281728
373.151567	15518.269872	29.286746
372.872627	15539.697413	29.291764
373.733087	15539.037909	29.296781
373.763848	15587.279461	29.301799
374.200173	15614.092340	29.306816
374.927936	15626.636519	29.311834
375.004100	15657.656636	29.316852
375.684600	15692.703943	29.321869
375.822030	15703.343614	29.326887
376.205478	15747.660728	29.331904
376.550912	15734.156295	29.336922
376.440485	15793.717772	29.341940
377.260073	15789.943404	29.346957
377.404647	15852.383817	29.351975
377.919088	15844.357658	29.356992
378.380847	15887.912048	29.362010
378.322086	15913.395828	29.367028
379.469329	15912.956221	29.372045
379.256829	15984.732043	29.377063
379.995765	15981.620270	29.382080
380.374520	16017.106093	29.387098
381.017321	16015.994135	29.392116
381.354426	16064.243875	29.397133
381.683903	16067.569386	29.402151
382.119507	16104.112709	29.407168
382.979966	16109.687690	29.412186
383.074496	16162.009777	29.417204
383.675022	16145.153263	29.422221
383.663697	16182.261898	29.427239
384.100400	16182.768241	29.432256
384.670253	16203.796743	29.437274
384.873481	16257.202840	29.442292
385.545990	16252.863702	29.447309
385.430097	16283.861458	29.452327
385.231337	16297.968559	29.457344
386.238787	16300.671809	29.462362
386.137211	16364.006831	29.467380
386.549519	16364.648938	29.472397
387.118101	16406.039278	29.477415
387.589725	16427.332717	29.482432
388.053853	16464.898288	29.487450
387.993497	16478.058632	29.492468
388.352090	16503.606399	29.497485
389.073382	16511.342580	29.502503
389.255976	16557.955922	29.507520
389.825678	16559.600971	29.512538
389.899416	16602.911378	29.517556
390.757093	16623.834960	29.522573
390.876430	16636.124794	29.527591
391.328206	16689.968712	29.532608
391.685345	16693.173827	29.537626
391.738952	16708.041187	29.542644
392.261637	16773.572822	29.547661
392.857940	16773.004086	29.552679
392.938523	16818.226765	29.557696
394.088883	16829.228011	29.562714
394.376936	16846.244309	29.567732
394.581001	16856.655684	29.572749
395.133298	16906.813119	29.577767
395.391524	16905.165104	29.582784
395.866575	16931.138283	29.587802
396.302713	16965.720894	29.592820
396.860361	16979.536465	29.597837
397.256092	17016.399790	29.602855
397.099896	17027.394805	29.607872
397.958011	17051.412867	29.612890
398.151197	17079.544174	29.617908
398.521237	17120.952520	29.622925
398.900611	17129.799097	29.627943
399.071681	17158.282658	29.632960
399.603706	17186.377299	29.637978
399.920106	17231.693329	29.642996
400.627400	17242.316887	29.648013
400.956871	17271.516887	29.653031
400.920570	17318.225268	29.658048
401.894859	17307.497963	29.663066
402.142274	17384.885455	29.668084
402.571977	17376.443703	29.673101
403.114927	17413.798651	29.678119
403.352131	17426.832873	29.683136
403.924714	17445.085501	29.688154
404.032824	17502.655814	29.693172
404.498406	17511.092843	29.698189
405.135455	17532.389211	29.703207
405.277636	17576.411074	29.708224
405.790789	17596.296070	29.713242
406.238444	17626.993360	29.718260
406.562152	17646.525756	29.723277
406.937077	17678.115385	29.728295
407.319926	17705.070442	29.733312
408.011359	17721.364425	29.738330
407.941716	17759.637445	29.743348
408.388283	17783.397633	29.748365
409.373045	17798.646990	29.753383
409.168401	17828.985049	29.758400
410.126350	17861.533487	29.763418
410.551616	17869.679516	29.768436
410.741540	17890.503351	29.773453
410.831490	17908.046847	29.778471
411.123164	17922.091066	29.783488
411.958653	17953.515563	29.788506
411.857177	17989.660068	29.793524
412.380610	17992.780898	29.798541
413.083811	18051.470789	29.803559
413.063625	18057.794654	29.808576
413.571237	18094.720283	29.813594
413.806959	18107.574023	29.818612
414.207001	18171.151469	29.823629
414.764851	18188.467198	29.828647
415.004801	18218.255278	29.833664
415.430723	18256.138372	29.838682
416.063119	18279.656338	29.843700
416.475056	18319.083509	29.848717
416.942159	18342.482631	29.853735
416.993434	18380.555243	29.858752
417.847562	18399.766884	29.863770
418.226964	18445.506539	29.868788
418.901653	18447.956920	29.873805
419.614129	18502.477809	29.878823
420.026452	18511.858117	29.883840
420.658089	18511.995706	29.888858
420.542362	18561.125575	29.893876
421.278621	18553.830800	29.898893
421.745858	18600.393921	29.903911
421.905145	18627.129508	29.908928
422.578930	18628.520617	29.913946
422.624490	18683.855873	29.918964
423.174059	18684.295122	29.923981
423.831574	18716.490078	29.928999
423.828611	18751.991523	29.934016
424.850472	18745.606678	29.939034
425.022739	18793.217769	29.944052
425.235871	18823.134118	29.949069
425.941806	18845.857757	29.954087
426.137203	18873.165580	29.959104
426.943234	18891.642577	29.964122
427.075592	18939.535673	29.969140
427.371385	18947.398171	29.974157
427.766875	18961.438606	29.979175
427.979627	19005.450521	29.984192
428.553454	19029.360463	29.989210
429.130743	19062.771309	29.994228
428.944558	19074.924544	29.999245
429.707046	19115.179802	30.004263
430.079007	19151.368118	30.009280
430.495180	19181.993384	30.014298
431.271611	19208.507633	30.019316
431.214642	19226.335087	30.024333
431.969477	19288.034923	30.029351
432.244068	19299.785384	30.034368
432.715920	19318.536218	30.039386
432.929807	19355.928194	30.044404
433.294587	19390.729172	30.049421
433.949277	19392.889971	30.054439
434.227646	19451.744966	30.059456
434.783636	19452.359215	30.064474
435.301862	19505.279841	30.069492
435.812571	19519.227620	30.074509
436.028525	19543.668620	30.079527
436.077416	19609.940321	30.084544
437.035863	19601.507637	30.089562
437.301548	19634.138201	30.094580
437.618421	19678.892957	30.099597
438.149477	19714.850530	30.104615
438.716811	19717.958034	30.109632
438.864647	19773.135574	30.114650
439.735295	19814.225079	30.119668
439.979325	19830.536264	30.124685
440.493264	19870.329887	30.129703
440.871578	19882.202465	30.134720
441.096218	19934.038945	30.139738
441.887404	19948.125119	30.144756
442.096498	19980.520520	30.149773
442.868211	20033.950636	30.154791
443.701035	20043.935024	30.159808
443.831815	20079.510316	30.164826
444.103617	20106.583698	30.169844
444.441126	20121.327791	30.174861
445.083620	20169.081181	30.179879
445.312556	20181.251433	30.184896
445.686795	20216.520115	30.189914
446.366402	20259.651664	30.194932
446.469048	20286.259341	30.199949
447.152437	20316.296180	30.204967
447.627102	20361.586081	30.209984
448.366010	20382.456125	30.215002
448.563024	20404.915840	30.220020
449.044912	20450.326120	30.225037
449.827193	20480.438476	30.230055
449.917744	20502.032511	30.235072
450.528077	20524.842746	30.240090
450.826522	20559.486799	30.245108
451.198308	20604.641018	30.250125
451.787767	20617.314483	30.255143
452.185965	20656.857254	30.260160
452.787413	20693.146855	30.265178
452.781393	20729.601038	30.270196
453.406775	20764.033204	30.275213
453.870935	20787.188805	30.280231
454.139322	20826.841672	30.285248
454.880594	20850.333983	30.290266
455.431167	20878.948373	30.295284
455.670029	20904.367518	30.300301
456.398648	20948.272012	30.305319
457.025033	20971.382749	30.310336
457.319035	20993.122635	30.315354
457.691947	21014.486541	30.320372
457.986840	21058.224180	30.325389
458.578445	21065.238932	30.330407
458.751767	21081.843833	30.335424
459.401468	21117.564047	30.340442
460.202216	21150.512602	30.345460
460.238395	21174.635128	30.350477
460.722862	21191.636321	30.355495
461.470151	21223.271284	30.360512
461.798259	21258.473666	30.365530
462.258133	21267.283016	30.370548
462.548055	21312.426326	30.375565
463.062766	21338.909507	30.380583
463.236475	21362.310293	30.385600
463.725112	21414.787291	30.390618
464.541040	21433.378755	30.395636
464.305931	21471.662413	30.400653
464.967165	21501.012021	30.405671
465.636803	21549.581195	30.410688
465.761945	21572.850635	30.415706
466.574515	21585.490531	30.420724
466.572684	21647.547422	30.425741
467.576506	21700.960037	30.430759
467.920082	21717.666861	30.435776
468.281815	21776.906755	30.440794
468.846584	21787.790657	30.445812
469.247561	21831.808884	30.450829
469.505049	21872.054827	30.455847
470.317072	21886.789184	30.460864
470.618798	21948.485454	30.465882
471.701264	21967.578517	30.470900
471.839702	22002.660777	30.475917
472.558711	22034.236515	30.480935
472.790493	22081.494106	30.485952
473.455677	22101.240545	30.490970
473.757815	22130.375245	30.495988
474.501015	22169.553019	30.501005
475.089068	22185.752790	30.506023
475.544059	22215.550067	30.511040
476.410766	22259.314947	30.516058
476.803596	22267.790582	30.521076
477.255029	22291.929793	30.526093
477.702468	22349.157724	30.531111
477.981581	22355.438403	30.536128
478.531882	22356.357313	30.541146
479.017769	22424.155111	30.546164
479.365116	22406.933507	30.551181
480.078371	22466.955633	30.556199
480.144678	22472.477940	30.561216
480.734533	22531.455930	30.566234
480.821129	22536.960063	30.571252
481.343782	22601.910335	30.576269
481.632319	22617.273788	30.581287
482.200314	22649.167016	30.586304
482.393634	22677.307205	30.591322
482.867295	22729.244373	30.596340
483.475752	22737.937162	30.601357
483.798575	22800.903024	30.606375
484.296518	22809.912749	30.611392
484.615184	22870.576580	30.616410
485.620519	22887.508459	30.621428
485.495686	22935.624051	30.626445
486.246938	22983.601813	30.631463
486.651401	23023.657155	30.636480
487.283873	23035.317188	30.641498
487.755725	23101.084913	30.646516
488.428890	23091.655405	30.651533
489.038056	23161.991782	30.656551
489.372187	23195.557692	30.661568
489.980026	23218.752671	30.666586
490.524836	23276.001528	30.671604
490.946997	23280.660112	30.676621
491.327482	23304.222237	30.681639
491.516601	23394.055917	30.686656
492.085066	23411.788880	30.691674
492.672993	23460.257236	30.696692
493.054412	23484.870983	30.701709
493.824823	23539.531320	30.706727
494.107683	23556.166276	30.711744
494.365624	23614.245758	30.716762
495.646967	23629.745851	30.721780
495.566669	23663.222022	30.726797
496.503690	23726.026778	30.731815
496.847783	23749.446496	30.736832
496.993533	23789.475670	30.741850
497.835229	23811.140083	30.746868
498.171507	23884.509148	30.751885
498.750828	23901.814807	30.756903
499.020425	23944.708282	30.761920
499.698437	24000.539645	30.766938
500.645380	24022.546761	30.771956
500.888333	24089.839017	30.776973
501.528997	24097.798836	30.781991
502.095649	24135.553992	30.787008
502.442575	24176.829707	30.792026
503.028414	24199.040308	30.797044
503.563807	24250.982871	30.802061
503.934084	24271.634430	30.807079
504.734251	24314.501107	30.812096
504.748508	24362.034091	30.817114
505.701765	24365.929420	30.822132
505.848940	24444.378684	30.827149
506.461869	24444.006184	30.832167
506.835477	24517.393490	30.837184
507.310172	24527.349199	30.842202
507.978152	24595.992957	30.847220
508.445105	24601.706618	30.852237
509.132775	24640.525209	30.857255
509.588173	24710.461278	30.862272
509.565501	24722.990988	30.867290
510.286672	24729.497595	30.872308
510.559400	24803.334735	30.877325
511.056580	24830.869496	30.882343
511.930358	24837.256528	30.887360
512.564455	24863.855796	30.892378
512.872091	24940.124399	30.897396
513.056026	24948.143219	30.902413
514.183361	25017.809768	30.907431
514.101754	25027.442422	30.912448
515.065217	25045.482168	30.917466
515.647908	25090.990570	30.922484
515.811633	25172.660987	30.927501
516.326681	25198.970200	30.932519
516.890564	25243.483194	30.937536
517.457279	25284.937097	30.942554
517.775044	25299.168101	30.947572
518.486188	25334.460331	30.952589
519.468583	25339.846392	30.957607
519.689218	25388.158563	30.962624
520.317830	25463.694000	30.967642
520.771983	25504.851307	30.972660
521.240359	25549.047150	30.977677
521.739417	25587.325400	30.982695
522.078743	25600.866325	30.987712
522.440791	25637.757238	30.992730
523.760395	25657.183329	30.997748
523.926179	25689.041175	31.002765
524.253583	25742.782352	31.007783
525.090884	25810.720599	31.012800
525.159323	25831.490005	31.017818
526.361116	25851.206087	31.022836
526.106183	25945.189704	31.027853
526.672167	25957.084641	31.032871
527.801684	25959.707641	31.037888
527.725167	26046.441994	31.042906
528.838421	26084.783529	31.047924
529.087582	26107.113442	31.052941
529.819062	26131.361997	31.057959
530.089544	26203.759607	31.062976
530.322200	26215.447861	31.067994
531.208328	26269.710770	31.073012
531.185407	26298.596077	31.078029
532.216366	26328.899392	31.083047
532.938214	26408.339719	31.088064
533.270152	26434.351626	31.093082
533.842792	26476.779808	31.098100
534.507192	26500.664620	31.103117
534.956623	26577.334392	31.108135
535.482991	26591.530174	31.113152
535.886930	26624.025513	31.118170
536.528908	26676.982341	31.123188
537.402045	26693.212231	31.128205
537.700693	26762.304623	31.133223
538.574692	26767.404356	31.138240
538.770057	26818.406548	31.143258
539.455945	26842.969115	31.148276
539.765058	26882.689316	31.153293
540.266552	26918.620323	31.158311
540.534697	26931.894828	31.163328
541.059387	27001.536016	31.168346
541.664443	27015.805516	31.173364
542.253982	27067.115992	31.178381
542.651258	27099.904848	31.183399
543.186963	27139.346946	31.188416
543.543544	27191.994830	31.193434
544.088766	27214.564325	31.198452
544.590677	27267.104223	31.203469
545.089032	27317.657948	31.208487
545.955813	27360.819998	31.213504
546.483667	27402.343084	31.218522
546.937464	27440.500612	31.223540
547.702678	27494.946854	31.228557
548.188103	27538.059818	31.233575
548.891120	27566.257446	31.238592
549.461486	27622.080788	31.243610
549.884261	27660.534493	31.248628
550.797642	27695.850145	31.253645
551.298045	27737.192535	31.258663
551.943453	27772.779511	31.263680
552.206224	27815.136884	31.268698
552.894793	27848.046323	31.273716
553.476948	27894.642135	31.278733
553.928734	27930.967796	31.283751
554.559740	27965.035343	31.288768
554.872852	28019.660146	31.293786
555.381267	28064.872096	31.298804
555.687332	28098.206958	31.303821
556.145312	28133.767855	31.308839
557.433473	28195.220083	31.313856
557.736706	28229.165481	31.318874
558.266282	28287.831612	31.323892
558.825559	28328.551594	31.328909
559.349505	28353.946691	31.333927
559.945820	28413.565440	31.338944
560.611725	28466.123308	31.343962
561.191780	28498.742506	31.348980
561.699689	28542.302881	31.353997
562.025738	28585.963246	31.359015
563.243654	28634.658167	31.364032
563.219777	28663.760588	31.369050
563.891110	28733.945304	31.374068
564.695413	28752.690624	31.379085
564.854177	28801.423933	31.384103
565.935857	28848.757637	31.389120
565.983791	28911.702271	31.394138
566.867417	28936.943304	31.399156
567.488923	28996.572795	31.404173
567.937613	29025.372111	31.409191
568.753080	29028.471151	31.414208
568.962321	29105.261304	31.419226
569.191466	29128.529912	31.424244
569.838455	29164.324564	31.429261
570.016845	29221.455250	31.434279
571.017484	29245.303991	31.439296
571.413144	29326.186349	31.444314
572.171701	29330.690724	31.449332
572.768349	29388.672539	31.454349
573.432095	29429.851415	31.459367
573.711895	29469.846600	31.464384
574.427684	29504.737528	31.469402
574.639383	29540.928539	31.474420
575.086478	29607.848127	31.479437
575.452143	29661.639600	31.484455
576.397580	29700.323792	31.489472
576.820020	29749.266942	31.494490
577.471110	29817.034257	31.499508
578.410911	29864.280060	31.504525
578.982735	29899.658081	31.509543
579.878696	29966.611674	31.514560
580.148020	29990.527548	31.519578
580.958146	30055.952350	31.524596
581.597847	30072.136167	31.529613
582.188333	30138.294413	31.534631
582.953753	30169.395043	31.539648
583.080519	30227.295506	31.544666
584.202048	30255.078960	31.549684
584.992580	30291.196796	31.554701
585.263660	30353.055577	31.559719
586.044419	30372.012980	31.564736
586.309817	30424.037376	31.569754
586.887637	30477.444742	31.574772
587.811513	30518.179926	31.579789
588.167811	30541.947227	31.584807
588.485081	30605.169131	31.589824
589.232710	30623.927227	31.594842
589.443631	30692.085048	31.599860
590.570309	30714.614120	31.604877
590.589542	30776.793562	31.609895
591.953918	30816.789547	31.614912
592.486719	30854.809359	31.619930
592.994798	30917.991056	31.624948
593.777076	30933.489528	31.629965
594.120263	30973.457820	31.634983
594.491129	31046.519854	31.640000
595.281628	31065.566351	31.645018
595.762494	31136.787809	31.650036
596.892295	31149.750473	31.655053
596.806852	31227.852064	31.660071
597.685948	31252.905153	31.665088
598.152610	31291.541715	31.670106
598.575414	31343.740976	31.675124
599.293239	31395.445824	31.680141
600.191944	31435.098253	31.685159
600.448831	31479.155641	31.690176
601.103060	31515.299472	31.695194
601.516049	31556.555177	31.700212
602.326803	31596.642815	31.705229
602.687005	31620.708943	31.710247
603.183847	31689.911303	31.715264
603.842342	31724.533993	31.720282
604.394284	31743.472697	31.725300
605.042634	31787.325152	31.730317
605.694766	31879.577637	31.735335
606.394911	31917.540174	31.740352
606.849248	31922.007049	31.745370
607.324872	31998.784140	31.750388
607.381838	32041.937085	31.755405
608.304780	32069.556676	31.760423
609.049665	32149.235790	31.765440
609.481974	32223.997079	31.770458
609.956822	32258.911781	31.775476
610.718935	32287.900222	31.780493
611.615096	32331.531839	31.785511
612.073856	32405.596236	31.790528
613.148932	32484.470995	31.795546
613.261164	32502.943124	31.800564
614.487845	32529.277837	31.805581
614.333135	32624.979234	31.810599
615.489817	32638.060181	31.815616
616.044178	32727.223191	31.820634
616.661685	32740.397957	31.825652
617.143564	32823.752175	31.830669
617.426889	32861.026691	31.835687
618.330214	32914.790521	31.840704
619.207164	32966.698801	31.845722
619.797284	33036.156774	31.850740
620.829187	33041.531313	31.855757
621.141355	33137.229113	31.860775
621.636761	33154.595921	31.865792
622.682269	33188.591058	31.870810
623.104712	33283.299610	31.875828
623.625926	33294.792547	31.880845
624.412601	33345.747009	31.885863
624.734389	33428.114668	31.890880
625.554552	33455.406185	31.895898
626.053102	33511.096395	31.900916
626.942622	33552.654799	31.905933
627.468976	33632.664338	31.910951
628.026007	33651.432622	31.915968
629.023816	33723.330114	31.920986
629.410464	33748.046147	31.926004
629.955512	33797.287651	31.931021
630.691997	33855.449007	31.936039
631.451926	33865.793048	31.941056
632.110493	33959.591454	31.946074
632.539830	33975.008728	31.951092
633.551256	34044.786898	31.956109
634.141366	34062.691294	31.961127
634.574685	34133.603831	31.966144
635.361228	34128.267314	31.971162
635.492496	34221.281033	31.976180
636.301207	34252.497599	31.981197
636.644923	34291.851210	31.986215
636.928522	34318.937972	31.991232
637.964338	34339.511375	31.996250
638.142360	34445.361340	32.001268
639.147051	34454.047871	32.006285
639.539273	34538.041352	32.011303
639.849456	34582.689672	32.016320
641.110270	34608.148988	32.021338
641.164312	34697.602474	32.026356
642.274221	34719.168704	32.031373
642.610892	34809.826281	32.036391
643.533472	34845.772327	32.041408
644.309342	34920.673961	32.046426
644.733805	34936.155964	32.051444
645.479324	35005.375179	32.056461
646.167805	35057.662114	32.061479
646.929496	35119.618302	32.066496
647.496227	35159.505968	32.071514
647.970997	35210.758601	32.076532
648.505516	35284.692968	32.081549
649.110830	35328.889582	32.086567
649.911997	35403.663247	32.091584
650.765575	35444.565292	32.096602
651.496662	35495.100118	32.101620
652.168424	35544.466933	32.106637
652.821654	35602.229906	32.111655
653.598969	35643.037383	32.116672
654.293505	35703.447315	32.121690
654.881056	35740.143864	32.126708
655.613221	35800.158768	32.131725
655.870179	35863.985812	32.136743
656.866442	35910.267315	32.141760
657.604280	35955.551185	32.146778
657.889243	36017.564545	32.151796
658.909745	36080.061672	32.156813
659.499583	36120.710988	32.161831
660.179924	36175.605540	32.166848
660.589961	36230.256382	32.171866
661.408409	36301.115250	32.176884
662.041961	36343.233774	32.181901
662.704221	36396.009921	32.186919
663.855338	36448.957496	32.191936
664.397056	36487.480734	32.196954
664.615274	36563.271530	32.201972
665.679512	36612.506495	32.206989
666.317786	36661.041641	32.212007
666.614990	36710.695410	32.217024
667.792176	36769.734842	32.222042
668.358361	36797.058116	32.227060
668.874384	36875.774745	32.232077
669.758250	36898.059314	32.237095
670.241565	36970.959288	32.242112
671.198093	36996.391900	32.247130
671.237601	37035.292755	32.252148
671.570993	37111.364088	32.257165
672.489770	37121.396373	32.262183
673.046063	37204.355495	32.267200
673.940049	37245.812066	32.272218
674.068653	37292.489375	32.277236
674.734003	37373.913688	32.282253
675.595199	37407.224732	32.287271
676.321676	37452.661091	32.292288
677.320361	37522.599324	32.297306
677.689855	37589.536760	32.302324
678.326450	37618.557671	32.307341
678.898919	37684.435195	32.312359
679.457821	37758.564223	32.317376
680.637342	37793.326336	32.322394
681.137960	37885.618919	32.327412
682.036493	37919.044864	32.332429
682.758968	37976.756123	32.337447
683.208401	38034.608804	32.342464
683.878232	38074.859106	32.347482
684.563034	38157.665293	32.352500
685.237071	38201.399730	32.357517
686.303579	38249.923322	32.362535
686.680551	38324.039652	32.367552
687.923245	38343.196009	32.372570
688.022551	38444.139175	32.377588
688.901417	38465.586237	32.382605
689.478304	38539.618077	32.387623
690.022369	38619.069994	32.392640
690.975976	38673.774686	32.397658
691.425772	38718.815445	32.402676
692.115784	38793.795359	32.407693
693.041373	38854.047397	32.412711
693.220157	38921.975995	32.417728
694.465819	38961.354662	32.422746
694.994955	39057.307216	32.427764
695.890491	39084.345259	32.432781
696.910447	39159.226962	32.437799
697.535067	39207.771627	32.442816
698.434448	39269.634497	32.447834
699.036736	39318.790103	32.452852
699.488818	39361.645180	32.457869
700.474759	39430.251488	32.462887
701.198921	39480.649615	32.467904
702.045513	39510.512337	32.472922
702.502639	39604.831672	32.477940
702.733906	39637.581993	32.482957
703.867240	39667.563335	32.487975
704.251007	39742.552050	32.492992
705.125264	39838.862483	32.498010
705.671890	39868.995928	32.503028
706.533570	39940.060325	32.508045
707.712956	39947.097793	32.513063
707.857369	40031.440425	32.518080
708.448622	40077.690659	32.523098
709.127827	40110.099358	32.528116
709.828691	40189.719742	32.533133
710.219695	40219.303021	32.538151
710.631853	40299.319946	32.543168
711.886574	40330.158318	32.548186
712.115284	40423.443107	32.553204
712.942342	40479.321767	32.558221
714.030005	40529.395488	32.563239
714.617655	40582.381109	32.568256
714.858136	40655.378192	32.573274
715.408891	40689.169334	32.578292
716.339218	40796.681948	32.583309
717.173929	40832.389888	32.588327
717.714759	40925.558347	32.593344
718.921933	40970.678475	32.598362
719.451138	41032.225068	32.603380
719.988456	41112.262151	32.608397
721.143634	41161.093792	32.613415
721.592810	41235.562988	32.618432
722.285489	41301.840710	32.623450
723.045878	41357.876368	32.628468
723.936467	41443.195312	32.633485
724.518543	41493.617288	32.638503
724.651825	41573.935321	32.643520
726.301155	41631.344300	32.648538
726.664513	41707.819410	32.653556
727.493243	41766.239453	32.658573
727.982612	41846.338065	32.663591
729.214150	41875.626400	32.668608
730.028212	41977.228957	32.673626
730.791189	42003.557855	32.678644
731.312111	42107.286403	32.683661
732.347616	42147.977041	32.688679
732.943122	42226.133354	32.693696
733.826660	42287.769991	32.698714
734.429445	42349.984596	32.703732
734.987488	42418.426596	32.708749
735.999470	42451.706218	32.713767
736.525869	42560.716743	32.718784
737.153532	42585.257561	32.723802
737.972456	42685.734325	32.728820
738.587132	42728.732837	32.733837
739.529687	42799.521831	32.738855
739.988996	42888.301126	32.743872
741.083023	42909.389949	32.748890
741.941614	43027.384388	32.753908
742.268351	43062.140083	32.758925
743.462620	43108.703120	32.763943
743.714377	43193.037903	32.768960
744.662629	43250.330495	32.773978
745.312262	43324.152274	32.778996
746.665790	43360.972099	32.784013
747.214983	43461.382764	32.789031
747.479619	43496.663384	32.794048
748.543078	43576.479936	32.799066
748.762291	43621.474116	32.804084
749.858737	43652.559777	32.809101
750.350977	43753.082143	32.814119
750.801506	43791.191685	32.819136
751.786526	43859.360093	32.824154
752.228801	43928.457403	32.829172
753.305803	43987.817048	32.834189
753.872040	44062.453337	32.839207
754.722951	44135.574639	32.844224
755.299826	44191.639281	32.849242
756.347195	44258.991787	32.854260
756.809100	44320.541929	32.859277
757.820282	44415.648072	32.864295
758.545313	44465.245279	32.869312
759.403486	44554.509065	32.874330
759.804153	44614.028987	32.879348
760.898507	44673.063300	32.884365
761.801393	44735.248195	32.889383
762.293924	44828.019572	32.894400
763.412735	44874.662483	32.899418
764.219920	44962.409641	32.904436
764.954562	45038.146376	32.909453
765.495216	45083.888158	32.914471
766.610664	45145.523324	32.919488
766.736254	45236.355217	32.924506
767.924745	45272.322084	32.929524
768.543916	45388.796516	32.934541
769.640997	45421.645602	32.939559
770.315749	45513.041401	32.944576
771.131981	45584.688442	32.949594
771.615458	45648.129550	32.954612
772.781243	45708.714472	32.959629
773.528424	45769.227423	32.964647
774.233052	45859.733787	32.969664
775.135881	45895.056511	32.974682
775.948154	45997.386479	32.979700
776.226003	46036.146780	32.984717
777.405712	46120.045203	32.989735
778.157216	46198.686764	32.994752
779.029251	46252.379621	32.999770
779.974546	46317.027380	33.004788
780.434575	46403.732836	33.009805
781.352291	46457.217137	33.014823
782.356349	46533.867116	33.019840
782.916738	46607.720203	33.024858
783.737196	46664.470211	33.029876
784.250613	46765.158027	33.034893
785.635120	46782.775914	33.039911
786.223243	46904.556278	33.044928
786.486126	46932.770641	33.049946
787.711866	47032.071993	33.054964
788.437416	47081.152832	33.059981
789.339057	47143.068872	33.064999
790.009253	47208.277981	33.070016
790.722239	47254.240959	33.075034
791.405884	47323.723462	33.080052
791.945956	47398.860917	33.085069
792.725487	47451.190248	33.090087
793.498257	47517.466376	33.095104
794.008945	47586.630384	33.100122
795.024994	47646.501250	33.105140
795.785695	47724.927334	33.110157
796.739909	47798.432475	33.115175
797.552751	47852.079710	33.120192
798.421497	47946.691372	33.125210
799.421662	48004.811706	33.130228
799.858369	48069.070437	33.135245
800.798629	48142.822188	33.140263
801.538706	48221.752292	33.145280
802.152510	48277.644320	33.150298
802.935933	48373.455068	33.155316
803.730730	48434.793163	33.160333
804.487304	48506.004123	33.165351
804.986790	48578.660393	33.170368
805.815500	48681.038084	33.175386
806.812808	48732.490939	33.180404
807.643020	48826.450832	33.185421
808.879655	48910.801589	33.190439
809.459071	48972.033837	33.195456
810.171793	49050.602819	33.200474
811.482586	49121.197947	33.205492
811.691402	49206.773907	33.210509
812.818041	49284.120014	33.215527
813.474898	49369.739048	33.220544
814.358947	49443.804942	33.225562
815.391809	49508.027663	33.230580
815.893308	49601.116274	33.235597
816.937824	49661.254508	33.240615
817.815702	49741.011972	33.245632
818.577186	49817.238361	33.250650
819.757196	49886.513106	33.255668
820.218669	49967.577980	33.260685
820.938681	50052.448702	33.265703
822.129136	50128.112733	33.270720
822.920294	50197.617821	33.275738
823.757318	50270.337746	33.280756
824.052214	50356.142205	33.285773
825.401207	50435.622693	33.290791
826.230080	50505.930824	33.295808
826.783662	50591.647912	33.300826
827.653345	50677.769521	33.305844
828.301073	50756.397410	33.310861
829.359634	50818.828353	33.315879
829.989498	50907.286580	33.320896
830.743302	50996.498674	33.325914
832.017177	51062.979713	33.330932
832.512327	51138.689266	33.335949
833.430509	51214.237142	33.340967
834.370152	51285.622611	33.345984
834.893728	51358.942805	33.351002
836.022235	51422.693317	33.356020
836.568933	51495.495995	33.361037
837.471045	51568.327615	33.366055
838.284972	51636.761705	33.371072
838.931131	51730.179228	33.376090
840.109509	51775.111027	33.381108
840.815064	51861.119286	33.386125
841.677074	51929.442698	33.391143
842.333861	52000.623561	33.396160
843.094734	52090.335456	33.401178
843.898773	52146.695377	33.406196
844.575066	52247.495666	33.411213
845.461717	52322.892283	33.416231
846.388147	52407.043863	33.421248
847.126821	52504.550299	33.426266
848.333085	52581.295241	33.431284
848.685963	52658.226813	33.436301
849.527118	52760.698521	33.441319
850.835096	52836.194356	33.446336
851.428560	52922.051944	33.451354
852.382422	53015.240968	33.456372
853.269613	53093.604286	33.461389
854.103406	53175.236701	33.466407
855.039213	53283.487773	33.471424
855.557962	53337.147838	33.476442
856.571252	53461.130452	33.481460
856.983918	53546.117117	33.486477
858.750350	53621.025674	33.491495
859.398001	53707.424392	33.496512
860.523819	53797.774760	33.501530
861.377115	53864.724480	33.506548
862.138116	53976.615086	33.511565
863.161797	54039.334219	33.516583
863.870551	54120.703581	33.521600
864.655526	54219.714291	33.526618
865.887074	54285.529082	33.531636
866.518135	54368.774137	33.536653
867.536315	54457.756148	33.541671
868.493644	54545.886597	33.546688
869.250048	54623.519832	33.551706
870.113017	54699.324683	33.556724
870.761962	54796.800938	33.561741
871.865761	54881.229358	33.566759
872.924229	54965.324491	33.571776
873.987878	55044.665602	33.576794
875.231832	55107.848940	33.581812
875.891082	55173.729615	33.586829
876.434984	55280.634566	33.591847
877.510415	55349.568247	33.596864
878.031205	55428.634418	33.601882
878.728381	55521.517329	33.606900
879.789185	55603.396008	33.611917
880.051422	55688.375589	33.616935
881.656625	55752.267566	33.621952
882.210848	55816.456422	33.626970
883.087309	55934.215059	33.631988
883.440086	55997.906300	33.637005
884.720299	56066.087244	33.642023
885.691709	56149.731359	33.647040
886.971536	56195.724966	33.652058
887.785073	56321.346648	33.657076
888.206078	56364.282805	33.662093
888.686115	56463.868761	33.667111
889.632586	56522.473497	33.672128
890.295316	56656.556138	33.677146
891.533234	56705.092535	33.682164
892.367987	56825.123745	33.687181
893.483901	56882.862980	33.692199
894.325472	56987.653394	33.697216
895.023977	57086.065213	33.702234
896.334644	57137.258663	33.707252
897.027159	57270.040442	33.712269
898.429207	57317.198074	33.717287
898.907104	57430.572300	33.722304
899.709492	57502.319776	33.727322
900.720758	57591.722227	33.732340
901.632489	57694.472479	33.737357
902.042461	57776.391816	33.742375
903.406160	57872.492164	33.747392
903.951063	57950.340479	33.752410
904.925364	58053.265875	33.757428
905.398630	58157.054493	33.762445
906.806521	58254.071633	33.767463
907.550348	58350.509874	33.772480
908.769998	58422.671245	33.777498
909.715113	58562.478048	33.782516
910.463834	58660.160996	33.787533
911.431319	58731.571276	33.792551
913.044558	58810.411870	33.797568
913.326525	58943.305721	33.802586
914.617824	58993.926514	33.807604
915.195801	59125.937940	33.812621
916.641407	59178.312152	33.817639
917.394593	59296.424446	33.822656
918.295858	59362.202691	33.827674
919.395066	59475.818932	33.832692
920.577422	59552.871660	33.837709
921.231582	59639.789806	33.842727
922.106836	59743.788547	33.847744
923.106537	59815.235760	33.852762
924.204396	59919.247422	33.857780
924.667163	59988.507499	33.862797
925.791093	60104.216918	33.867815
926.483265	60174.896700	33.872832
927.412306	60289.949986	33.877850
928.357126	60361.373295	33.882868
929.368985	60462.572695	33.887885
930.275218	60542.540333	33.892903
931.447509	60617.736223	33.897920
932.107494	60699.003506	33.902938
932.946220	60777.072663	33.907956
933.876683	60857.366165	33.912973
934.638525	60937.251113	33.917991
935.890504	61036.681985	33.923008
936.270354	61104.614314	33.928026
937.439027	61191.546233	33.933044
938.394368	61285.995760	33.938061
939.291050	61362.653054	33.943079
940.060966	61459.340054	33.948096
940.950746	61565.588463	33.953114
941.837751	61651.386406	33.958132
942.670586	61760.685706	33.963149
943.629774	61862.321006	33.968167
944.771774	61931.186547	33.973184
945.038666	62048.825223	33.978202
946.533800	62148.785362	33.983220
947.555040	62252.654823	33.988237
948.191103	62337.002246	33.993255
949.213150	62445.220754	33.998272
950.294050	62544.453159	34.003290
951.369668	62631.968620	34.008308
952.055031	62753.893296	34.013325
952.971350	62860.773180	34.018343
954.029158	62957.425225	34.023360
954.959500	63070.834345	34.028378
956.150387	63171.252507	34.033396
957.104661	63280.497083	34.038413
958.206699	63392.216638	34.043431
959.351370	63472.660903	34.048448
960.025818	63573.573882	34.053466
961.227338	63676.459336	34.058484
962.415566	63778.532722	34.063501
963.244890	63881.036391	34.068519
964.444591	63967.606702	34.073536
964.959861	64074.130909	34.078554
966.293500	64166.883058	34.083572
967.489350	64266.734641	34.088589
967.921546	64368.388297	34.093607
969.032929	64479.051671	34.098624
970.123266	64583.993498	34.103642
971.174546	64665.474567	34.108660
972.200244	64771.542506	34.113677
973.115051	64877.865533	34.118695
974.114878	64955.923182	34.123712
974.901000	65074.663350	34.128730
975.861216	65153.542906	34.133748
976.982411	65274.125893	34.138765
978.187836	65362.097542	34.143783
979.512721	65456.610152	34.148800
979.871849	65550.607323	34.153818
980.976475	65628.496298	34.158836
981.982660	65752.536738	34.163853
982.717960	65841.640232	34.168871
983.829225	65926.164852	34.173888
984.427979	66025.391062	34.178906
985.423324	66119.634065	34.183924
986.343720	66215.174888	34.188941
986.998454	66304.245972	34.193959
988.201035	66387.422125	34.198976
988.993889	66506.593310	34.203994
990.257590	66579.243229	34.209012
991.082772	66685.233647	34.214029
991.859318	66817.421926	34.219047
993.391960	66891.647352	34.224064
993.971491	66995.398170	34.229082
994.925643	67093.565809	34.234100
996.434809	67212.671631	34.239117
997.255754	67302.321001	34.244135
998.593688	67397.734945	34.249152
999.191112	67512.047745	34.254170
1000.283095	67614.292716	34.259188
1001.264134	67711.900159	34.264205
1001.798393	67807.184966	34.269223
1003.145746	67917.401063	34.274240
1004.001842	68033.450922	34.279258
1004.742391	68146.891875	34.284276
1005.911868	68252.109634	34.289293
1007.064314	68370.192757	34.294311
1008.252689	68474.574828	34.299328
1009.224629	68594.090481	34.304346
1010.340860	68693.052237	34.309364
1011.422091	68798.166961	34.314381
1012.288127	68910.354187	34.319399
1013.590361	69012.598356	34.324416
1014.620542	69122.296852	34.329434
1015.303646	69235.260521	34.334452
1016.549356	69332.492860	34.339469
1017.195999	69439.632327	34.344487
1018.513604	69569.264127	34.349504
1019.480186	69672.342228	34.354522
1020.931227	69775.697609	34.359540
1021.905456	69893.135993	34.364557
1022.733539	70003.705542	34.369575
1024.060899	70103.222116	34.374592
1024.894327	70224.229221	34.379610
1026.016465	70321.865217	34.384628
1026.901578	70418.269485	34.389645
1028.039419	70548.296492	34.394663
1029.415034	70643.284423	34.399680
1029.865742	70749.963097	34.404698
1030.710367	70858.386679	34.409716
1032.289143	70964.646998	34.414733
1033.294323	71087.167417	34.419751
1034.405611	71168.653700	34.424768
1035.299536	71297.467132	34.429786
1036.323545	71392.116559	34.434804
1037.409202	71491.495389	34.439821
1038.231399	71611.767256	34.444839
1039.453879	71703.202148	34.449856
1040.391257	71802.031152	34.454874
1041.563326	71894.586995	34.459892
1042.626491	71978.744359	34.464909
1043.283498	72079.041006	34.469927
1044.234104	72169.598797	34.474944
1045.631808	72265.955856	34.479962
1046.054457	72373.279625	34.484980
1047.081179	72470.126350	34.489997
1047.994925	72591.274223	34.495015
1049.375666	72696.115756	34.500032
1050.492393	72794.270362	34.505050
1051.250568	72898.118840	34.510068
1052.494825	73008.601135	34.515085
1053.524154	73137.379733	34.520103
1054.424501	73245.573747	34.525120
1055.687065	73348.118486	34.530138
1056.440242	73459.591320	34.535156
1057.485486	73593.318085	34.540173
1058.422004	73685.022454	34.545191
1059.701560	73815.585521	34.550208
1061.201384	73915.498307	34.555226
1062.023456	74029.421501	34.560244
1063.077431	74146.291115	34.565261
1064.099350	74266.067032	34.570279
1065.502345	74386.231724	34.575296
1066.727214	74495.448858	34.580314
1067.830047	74602.550065	34.585332
1068.754236	74727.254402	34.590349
1069.749003	74830.835174	34.595367
1071.168352	74938.665124	34.600384
1072.299593	75047.849606	34.605402
1073.073388	75171.455758	34.610420
1074.111729	75289.320369	34.615437
1075.234314	75408.575220	34.620455
1076.348639	75504.556960	34.625472
1077.621151	75617.684465	34.630490
1078.417017	75736.917388	34.635508
1079.830298	75850.390355	34.640525
1081.014183	75961.423102	34.645543
1081.434888	76086.715202	34.650560
1082.764743	76195.147546	34.655578
1083.656914	76309.274756	34.660596
1084.842383	76414.261638	34.665613
1085.634831	76543.687537	34.670631
1086.678094	76672.164299	34.675648
1088.061222	76792.574050	34.680666
1088.797995	76913.782516	34.685684
1090.240854	77037.571770	34.690701
1091.309051	77160.435425	34.695719
1092.347975	77292.475039	34.700736
1093.530320	77407.263825	34.705754
1094.461256	77516.493512	34.710772
1096.011455	77647.537689	34.715789
1096.786289	77758.695906	34.720807
1097.749706	77862.587944	34.725824
1099.314779	77971.776110	34.730842
1100.204076	78073.159181	34.735860
1101.210966	78189.023147	34.740877
1102.155692	78286.094239	34.745895
1103.239039	78405.922856	34.750912
1103.771838	78509.697057	34.755930
1105.200858	78631.260738	34.760948
1106.751100	78736.511317	34.765965
1107.531375	78857.440001	34.770983
1108.230172	78980.803179	34.776000
1109.670704	79098.588035	34.781018
1110.518332	79223.085695	34.786036
1112.015256	79327.715718	34.791053
1112.278276	79472.281579	34.796071
1113.677960	79576.694465	34.801088
1115.241809	79705.335097	34.806106
1115.793435	79849.212976	34.811124
1117.573524	79959.635433	34.816141
1118.479474	80098.363989	34.821159
1119.901996	80200.393384	34.826176
1120.981188	80356.403203	34.831194
1122.107329	80453.645334	34.836212
1123.340953	80608.513659	34.841229
1124.149400	80711.629339	34.846247
1125.630081	80860.265469	34.851264
1126.881099	80959.810030	34.856282
1127.501878	81080.517955	34.861300
1129.046959	81227.983360	34.866317
1130.219977	81341.392299	34.871335
1131.087083	81458.219835	34.876352
1132.404002	81609.308494	34.881370
1133.022000	81712.042218	34.886388
1134.677959	81850.960365	34.891405
1135.726194	81984.292955	34.896423
1137.264626	82085.788524	34.901440
1138.344569	82245.845643	34.906458
1139.135858	82348.554952	34.911476
1140.584000	82489.950594	34.916493
1142.170625	82596.959888	34.921511
1142.936710	82735.424868	34.926528
1144.674224	82862.154624	34.931546
1145.477959	82962.747148	34.936564
1146.525432	83097.996190	34.941581
1147.702103	83207.362343	34.946599
1148.925058	83336.180860	34.951616
1150.235601	83468.197844	34.956634
1151.209419	83577.983833	34.961652
1152.490946	83689.143946	34.966669
1153.473420	83816.726584	34.971687
1154.450662	83943.602742	34.976704
1155.662834	84044.388396	34.981722
1156.647744	84193.645538	34.986740
1158.020380	84324.368285	34.991757
1159.105651	84429.076826	34.996775
1160.330054	84546.610831	35.001792
1161.386739	84658.836045	35.006810
1162.254324	84773.431227	35.011828
1163.604435	84887.722698	35.016845
1164.574178	84996.435587	35.021863
1165.631064	85121.384123	35.026880
1167.095236	85226.618047	35.031898
1167.931951	85350.983334	35.036916
1168.868925	85471.097230	35.041933
1170.453958	85573.658150	35.046951
1171.476307	85711.476000	35.051968
1172.887372	85836.119526	35.056986
1173.722551	85972.141550	35.062004
1175.168189	86087.688868	35.067021
1176.074133	86188.798997	35.072039
1177.100973	86345.215799	35.077056
1178.375497	86469.872104	35.082074
1179.609978	86592.202324	35.087092
1180.652557	86725.439359	35.092109
1181.760177	86860.848341	35.097127
1183.016962	86990.214869	35.102144
1184.311917	87114.283642	35.107162
1185.104799	87273.121939	35.112180
1186.693652	87394.306497	35.117197
1188.194394	87525.452238	35.122215
1189.320563	87658.194900	35.127232
1190.428292	87798.504030	35.132250
1191.208534	87935.160643	35.137268
1192.637412	88068.382553	35.142285
1194.006594	88209.898513	35.147303
1195.069451	88337.318435	35.152320
1196.711789	88469.111395	35.157338
1197.879147	88611.863559	35.162356
1198.990100	88742.465314	35.167373
1200.252051	88874.163140	35.172391
1201.235978	89017.446718	35.177408
1202.799543	89140.188123	35.182426
1203.681202	89278.411732	35.187444
1205.026818	89407.007176	35.192461
1206.324240	89548.088006	35.197479
1207.576163	89684.592165	35.202496
1208.987788	89812.730527	35.207514
1210.099206	89940.930023	35.212532
1211.386488	90083.862547	35.217549
1212.739821	90200.894863	35.222567
1214.021833	90329.607074	35.227584
1215.047562	90478.326039	35.232602
1216.406987	90597.313673	35.237620
1217.672652	90721.806263	35.242637
1218.746684	90854.861418	35.247655
1219.806448	90992.245454	35.252672
1221.212200	91133.205503	35.257690
1222.617056	91258.861674	35.262708
1223.814557	91390.319372	35.267725
1224.945597	91492.088946	35.272743
1226.268706	91621.150081	35.277760
1227.441395	91738.959326	35.282778
1228.411142	91866.370470	35.287796
1229.731109	91969.965314	35.292813
1230.761850	92094.610580	35.297831
1231.526220	92199.483857	35.302848
1233.074836	92342.370628	35.307866
1234.065109	92456.057416	35.312884
1235.033952	92598.519395	35.317901
1236.558442	92737.851743	35.322919
1237.615462	92846.874903	35.327936
1238.806157	92994.433586	35.332954
1239.912744	93136.554572	35.337972
1241.509110	93248.049226	35.342989
1242.579101	93409.804019	35.348007
1243.769403	93518.474080	35.353024
1245.301453	93674.951884	35.358042
1246.108847	93806.264636	35.363060
1247.519972	93967.981920	35.368077
1248.944099	94102.607625	35.373095
1250.171170	94234.166123	35.378112
1251.467288	94361.887655	35.383130
1252.844550	94524.936348	35.388148
1254.107428	94652.993748	35.393165
1255.236467	94790.365109	35.398183
1256.514392	94945.734710	35.403200
1258.040845	95071.374261	35.408218
1258.941091	95209.885198	35.413236
1260.298109	95362.316426	35.418253
1261.577276	95513.413722	35.423271
1262.970344	95645.890336	35.428288
1264.461460	95783.153306	35.433306
1265.257736	95937.695462	35.438324
1266.839216	96075.951641	35.443341
1268.235119	96213.498057	35.448359
1269.138618	96360.802060	35.453376
1270.715620	96510.865571	35.458394
1272.220754	96640.635428	35.463412
1273.251745	96792.660070	35.468429
1274.613060	96948.719799	35.473447
1276.056701	97093.829855	35.478464
1277.331757	97220.495595	35.483482
1278.183568	97385.628634	35.488500
1279.893264	97521.545297	35.493517
1281.310062	97638.790227	35.498535
1282.199354	97798.498800	35.503552
1283.722919	97954.349883	35.508570
1285.309620	98076.403320	35.513588
1286.353397	98240.145584	35.518605
1288.177609	98354.836882	35.523623
1289.217387	98494.996971	35.528640
1290.586408	98647.075203	35.533658
1291.799275	98769.261370	35.538676
1293.153096	98922.153640	35.543693
1294.625721	99028.629140	35.548711
1295.656369	99156.736357	35.553728
1296.862409	99283.778847	35.558746
1298.374081	99408.457910	35.563764
1299.375588	99526.347967	35.568781
1300.397482	99649.847184	35.573799
1301.640685	99804.755846	35.578816
1302.555911	99908.091063	35.583834
1304.092260	100065.985422	35.588852
1305.262666	100176.645715	35.593869
1306.859019	100338.296888	35.598887
1307.895131	100460.140549	35.603904
1309.042802	100615.816434	35.608922
1310.479619	100726.740721	35.613940
1311.497362	100901.818822	35.618957
1312.662704	101015.312141	35.623975
1313.846320	101201.944722	35.628992
1315.623443	101318.708330	35.634010
1316.691617	101503.412920	35.639028
1317.966879	101635.981043	35.644045
1320.149422	101748.392501	35.649063
1320.731843	101943.035709	35.654080
1322.198982	102086.155221	35.659098
1323.674120	102244.396877	35.664116
1324.660016	102389.353765	35.669133
1326.568355	102528.970064	35.674151
1327.495653	102684.194976	35.679168
1329.050195	102855.209793	35.684186
1330.733087	102980.855355	35.689204
1331.718274	103169.654998	35.694221
1333.160412	103279.103625	35.699239
1334.432709	103476.427817	35.704256
1335.953840	103584.384621	35.709274
1337.252366	103782.219764	35.714292
1338.438941	103920.826400	35.719309
1339.964663	104053.450699	35.724327
1341.093516	104232.541692	35.729344
1342.844731	104358.221741	35.734362
1344.177809	104535.371523	35.739380
1345.509723	104662.961296	35.744397
1347.079896	104839.101150	35.749415
1348.753349	104966.429454	35.754432
1349.827631	105137.391645	35.759450
1351.631453	105254.695900	35.764468
1352.454634	105420.738707	35.769485
1354.044376	105543.856133	35.774503
1355.013154	105736.785989	35.779520
1356.598268	105853.976087	35.784538
1357.672515	106029.431530	35.789556
1359.402505	106148.650469	35.794573
1360.897930	106335.616002	35.799591
1362.069543	106474.353869	35.804608
1363.776207	106598.692240	35.809626
1365.291670	106780.747090	35.814644
1366.365230	106904.156097	35.819661
1368.014664	107016.917951	35.824679
1369.101147	107191.316757	35.829696
1370.089989	107326.816650	35.834714
1371.478184	107424.629065	35.839732
1373.059427	107551.713707	35.844749
1374.370304	107702.992975	35.849767
1375.708068	107827.168509	35.854784
1376.659403	107978.740817	35.859802
1378.287300	108079.789875	35.864820
1379.501333	108254.752056	35.869837
1380.689349	108390.568050	35.874855
1381.459316	108544.736001	35.879872
1383.226602	108690.246413	35.884890
1384.520381	108835.421551	35.889908
1385.605962	109010.181755	35.894925
1387.232172	109149.856490	35.899943
1388.521993	109331.415819	35.904960
1389.870516	109474.180943	35.909978
1391.742285	109634.839196	35.914996
1393.187589	109793.775053	35.920013
1394.853275	109931.960597	35.925031
1395.867602	110109.619923	35.930048
1397.570514	110233.540888	35.935066
1398.902298	110416.671357	35.940084
1400.194507	110554.577976	35.945101
1402.056796	110714.985334	35.950119
1403.498069	110860.408616	35.955136
1404.786998	111023.782790	35.960154
1406.001588	111193.980711	35.965172
1407.634463	111322.108635	35.970189
1408.878394	111517.211975	35.975207
1409.984620	111660.414478	35.980224
1411.587115	111830.320951	35.985242
1413.223116	111973.010650	35.990260
1414.353664	112152.457661	35.995277
1415.683145	112305.940054	36.000295
1416.825052	112467.593725	36.005312
1418.782278	112606.475952	36.010330
1420.492359	112809.143242	36.015348
1421.717588	112952.942014	36.020365
1423.615423	113139.218513	36.025383
1424.908137	113295.947645	36.030400
1426.594353	113421.628138	36.035418
1428.212068	113605.945917	36.040436
1428.843927	113756.294291	36.045453
1430.765765	113897.702541	36.050471
1432.255196	114075.909944	36.055488
1433.296283	114254.993835	36.060506
1434.680402	114378.625400	36.065524
1436.468691	114543.614679	36.070541
1437.872421	114736.014691	36.075559
1439.098134	114870.062503	36.080576
1440.431572	115022.915248	36.085594
1442.144856	115197.670106	36.090612
1443.452056	115364.944333	36.095629
1444.936557	115500.714357	36.100647
1446.251849	115663.203132	36.105664
1447.867508	115793.458656	36.110682
1449.232163	115937.543617	36.115700
1450.307274	116098.737512	36.120717
1451.563867	116220.239496	36.125735
1453.045042	116395.248437	36.130752
1454.646646	116525.883497	36.135770
1455.956482	116699.896116	36.140788
1457.233122	116866.646960	36.145805
1458.839284	117004.697611	36.150823
1460.200794	117180.357758	36.155840
1461.300834	117311.981917	36.160858
1463.076445	117494.910112	36.165876
1464.748270	117632.656154	36.170893
1466.064405	117843.112835	36.175911
1467.455316	118000.976221	36.180928
1469.035758	118133.617296	36.185946
1470.657393	118283.752957	36.190964
1471.989861	118499.284004	36.195981
1473.503996	118674.271649	36.200999
1475.105261	118845.453948	36.206016
1476.226538	119018.176275	36.211034
1477.882649	119178.144876	36.216052
1479.499019	119348.821569	36.221069
1480.988017	119502.588210	36.226087
1482.610370	119654.973218	36.231104
1483.910409	119841.197581	36.236122
1485.638665	120037.543425	36.241140
1487.219430	120194.820179	36.246157
1488.641749	120341.383865	36.251175
1490.448824	120499.538324	36.256192
1492.108258	120671.483289	36.261210
1493.738151	120821.955297	36.266228
1494.995648	120992.927755	36.271245
1496.606207	121155.410659	36.276263
1498.259389	121372.877598	36.281280
1499.338479	121526.860615	36.286298
1501.261152	121651.936141	36.291316
1502.575721	121878.389725	36.296333
1503.856504	122015.461281	36.301351
1505.525033	122194.342515	36.306368
1506.799072	122376.365255	36.311386
1509.052872	122518.338234	36.316404
1510.212416	122735.147596	36.321421
1511.623027	122876.319217	36.326439
1513.632905	123014.496010	36.331456
1514.608361	123233.415820	36.336474
1516.474445	123348.578612	36.341492
1517.682731	123558.547544	36.346509
1519.067380	123695.205997	36.351527
1520.890986	123891.552790	36.356544
1522.289770	124076.847827	36.361562
1523.380607	124224.511697	36.366580
1525.151877	124389.370146	36.371597
1526.610017	124565.957551	36.376615
1528.049313	124763.689081	36.381632
1529.439163	124902.556810	36.386650
1531.168807	125041.409280	36.391668
1532.225582	125216.025432	36.396685
1533.803637	125362.832852	36.401703
1535.697792	125497.228258	36.406720
1536.826235	125678.549320	36.411738
1538.513164	125853.778837	36.416756
1539.876893	126037.978292	36.421773
1541.437304	126216.624973	36.426791
1542.983826	126390.942920	36.431808
1544.196776	126575.055972	36.436826
1545.854140	126723.986259	36.441844
1547.598265	126868.508050	36.446861
1548.933720	127091.366912	36.451879
1550.708162	127260.650632	36.456896
1551.892372	127419.654479	36.461914
1553.380530	127587.186915	36.466932
1554.818275	127803.866235	36.471949
1556.153262	127958.782944	36.476967
1558.149180	128171.867546	36.481984
1559.890699	128354.679853	36.487002
1561.845966	128518.533427	36.492020
1563.139177	128743.680008	36.497037
1564.484892	128907.886081	36.502055
1566.323150	129085.544595	36.507072
1568.143806	129269.465209	36.512090
1569.900490	129436.332841	36.517108
1571.487843	129673.893334	36.522125
1573.286311	129849.409423	36.527143
1574.708938	130004.463052	36.532160
1576.339879	130174.838986	36.537178
1578.259915	130342.268882	36.542196
1579.563485	130526.584009	36.547213
1580.999649	130748.620265	36.552231
1582.433297	130905.083414	36.557248
1584.157757	131106.210740	36.562266
1585.555622	131296.495813	36.567284
1587.332405	131458.697408	36.572301
1589.286336	131665.518837	36.577319
1590.794486	131842.499864	36.582336
1592.458675	132003.113456	36.587354
1594.230785	132221.509838	36.592372
1595.892407	132379.883450	36.597389
1597.453335	132575.573919	36.602407
1598.906568	132744.802715	36.607424
1600.762694	132929.020482	36.612442
1602.479849	133106.280306	36.617460
1603.534977	133295.518316	36.622477
1605.334233	133480.470890	36.627495
1607.300520	133634.913359	36.632512
1608.138455	133847.705630	36.637530
1609.492358	134020.100045	36.642548
1611.729960	134198.715769	36.647565
1612.939997	134383.349641	36.652583
1614.514245	134564.150983	36.657600
1616.083935	134738.251335	36.662618
1617.750194	134897.487147	36.667636
1619.104280	135074.107264	36.672653
1620.399947	135253.715430	36.677671
1622.707040	135396.151823	36.682688
1623.633861	135592.850619	36.687706
1625.673611	135781.492481	36.692724
1627.248921	135952.874951	36.697741
1628.595265	136132.087710	36.702759
1630.189694	136329.737204	36.707776
1631.919661	136495.649575	36.712794
1633.440497	136717.452727	36.717812
1634.936040	136883.987435	36.722829
1636.833617	137060.786769	36.727847
1638.510942	137276.841659	36.732864
1639.802565	137449.874645	36.737882
1641.770548	137653.416931	36.742900
1643.616343	137838.770156	36.747917
1644.922598	138042.420224	36.752935
1647.071831	138205.842641	36.757952
1648.507273	138424.009962	36.762970
1650.130302	138614.066883	36.767988
1652.051485	138792.038751	36.773005
1653.551158	139029.551330	36.778023
1655.355947	139202.893287	36.783040
1656.887990	139383.984632	36.788058
1658.902059	139592.526045	36.793076
1660.378976	139785.895952	36.798093
1661.918575	139973.617649	36.803111
1663.564944	140179.433484	36.808128
1665.476398	140356.960026	36.813146
1667.190708	140586.416101	36.818164
1668.936258	140744.391022	36.823181
1670.897897	140971.276086	36.828199
1673.000636	141132.643514	36.833216
1674.738058	141350.188619	36.838234
1676.187730	141509.469230	36.843252
1678.146194	141732.659808	36.848269
1679.370773	141912.408448	36.853287
1681.299867	142079.701862	36.858304
1682.591438	142281.418668	36.863322
1684.678106	142456.889234	36.868340
1686.339662	142681.097164	36.873357
1687.999312	142833.798830	36.878375
1689.746935	143050.479977	36.883392
1691.246191	143231.663012	36.888410
1692.845980	143424.301573	36.893428
1694.673217	143629.009450	36.898445
1696.262077	143813.464411	36.903463
1697.803730	143997.522383	36.908480
1699.985617	144217.679068	36.913498
1701.452202	144383.423476	36.918516
1703.305198	144580.313182	36.923533
1704.752354	144763.148577	36.928551
1706.887784	144929.195313	36.933568
1708.204864	145111.292909	36.938586
1709.823639	145290.390333	36.943604
1712.019627	145449.179989	36.948621
1713.067024	145628.674290	36.953639
1714.648668	145802.710398	36.958656
1716.346248	146002.739285	36.963674
1717.949603	146167.520828	36.968692
1719.793393	146346.474507	36.973709
1721.465828	146535.698431	36.978727
1723.198784	146713.911258	36.983744
1724.509401	146927.786121	36.988762
1726.230649	147103.949516	36.993780
1728.269680	147281.356399	36.998797
1729.624576	147498.954865	37.003815
1731.432261	147680.761318	37.008832
1732.936518	147883.063862	37.013850
1734.758348	148090.666708	37.018868
1736.452821	148291.483867	37.023885
1738.004336	148485.568391	37.028903
1739.894739	148725.895344	37.033920
1741.901233	148900.197986	37.038938
1743.134580	149135.903926	37.043956
1745.433472	149325.197149	37.048973
1747.208184	149549.867359	37.053991
1749.447135	149757.490866	37.059008
1751.201268	149964.406702	37.064026
1752.740459	150159.454093	37.069044
1754.757446	150382.088641	37.074061
1756.289264	150579.687871	37.079079
1758.041314	150769.431358	37.084096
1760.087085	150978.994996	37.089114
1762.061554	151189.281249	37.094132
1763.817567	151397.346914	37.099149
1765.407126	151599.481781	37.104167
1767.301146	151793.392355	37.109184
1769.053000	152005.392679	37.114202
1770.957291	152212.375040	37.119220
1772.916404	152408.953978	37.124237
1774.263148	152629.745159	37.129255
1776.102485	152827.271114	37.134272
1778.025228	153045.564769	37.139290
1780.025272	153235.536731	37.144308
1781.864435	153443.386606	37.149325
1783.616219	153634.706150	37.154343
1785.554487	153863.792169	37.159360
1787.604781	154046.090221	37.164378
1789.255279	154246.989104	37.169396
1791.119799	154434.631178	37.174413
1792.879820	154642.843426	37.179431
1795.009772	154835.605935	37.184448
1796.690256	155030.330083	37.189466
1798.311763	155248.647940	37.194484
1800.337049	155430.665876	37.199501
1801.985877	155625.043469	37.204519
1803.770607	155807.849704	37.209536
1805.190019	155984.248408	37.214554
1806.781140	156149.450139	37.219572
1809.116798	156327.645147	37.224589
1810.263042	156512.014679	37.229607
1811.963994	156702.117136	37.234624
1813.792316	156888.624739	37.239642
1815.709246	157063.225613	37.244660
1817.338143	157257.691781	37.249677
1818.854957	157471.767409	37.254695
1820.728913	157633.989675	37.259712
1822.494899	157841.878237	37.264730
1824.527536	158022.666206	37.269748
1826.364659	158267.521477	37.274765
1827.222689	158468.482343	37.279783
1829.382757	158639.476766	37.284800
1831.179097	158912.709156	37.289818
1832.904667	159091.408441	37.294836
1834.933945	159316.040461	37.299853
1836.829345	159526.239142	37.304871
1838.794130	159745.608980	37.309888
1841.012287	159953.704709	37.314906
1843.096751	160163.230481	37.319924
1845.126962	160386.702576	37.324941
1846.865076	160587.054051	37.329959
1848.432522	160800.736318	37.334976
1850.998796	160997.078229	37.339994
1852.580046	161235.261132	37.345012
1855.061681	161414.651159	37.350029
1856.196388	161633.314836	37.355047
1858.500545	161849.448150	37.360064
1860.164983	162038.748517	37.365082
1861.845425	162287.676739	37.370100
1863.948907	162464.570366	37.375117
1865.400844	162697.089431	37.380135
1867.492264	162912.223017	37.385152
1869.143348	163105.792266	37.390170
1871.130241	163360.766642	37.395188
1873.271849	163546.587735	37.400205
1875.135591	163784.527140	37.405223
1877.326930	163983.303836	37.410240
1879.442055	164182.702471	37.415258
1880.750130	164434.710309	37.420276
1883.070976	164608.853202	37.425293
1884.864327	164835.650021	37.430311
1886.859550	165064.724453	37.435328
1888.844527	165265.265727	37.440346
1890.684148	165475.508161	37.445364
1892.273667	165677.103701	37.450381
1894.339942	165879.461754	37.455399
1896.534904	166118.606682	37.460416
1898.509484	166301.589219	37.465434
1900.346140	166544.497227	37.470452
1902.144854	166716.957304	37.475469
1904.049005	166901.171562	37.480487
1906.287244	167135.268202	37.485504
1907.937143	167291.659329	37.490522
1909.826075	167464.273426	37.495540
1911.424495	167669.531194	37.500557
1913.544819	167836.453408	37.505575
1915.129873	168026.621728	37.510592
1916.513367	168245.107785	37.515610
1918.834345	168425.635819	37.520628
1920.608832	168623.400061	37.525645
1922.344346	168833.652538	37.530663
1924.042739	169033.079904	37.535680
1925.841286	169239.861882	37.540698
1927.202836	169456.366982	37.545716
1929.831281	169661.598918	37.550733
1931.288429	169899.857514	37.555751
1933.400236	170095.723946	37.560768
1935.575591	170318.396221	37.565786
1937.349713	170554.363418	37.570804
1939.603315	170759.876340	37.575821
1941.249474	170985.363626	37.580839
1943.129274	171199.297397	37.585856
1945.363854	171441.869103	37.590874
1947.557599	171641.345531	37.595892
1949.440705	171870.301371	37.600909
1951.154276	172100.744231	37.605927
1953.564274	172315.158125	37.610944
1955.339420	172536.917163	37.615962
1957.361125	172782.905210	37.620980
1959.155875	172988.718316	37.625997
1961.448463	173238.928485	37.631015
1963.657597	173430.432433	37.636032
1965.730801	173675.669410	37.641050
1967.694959	173882.931796	37.646068
1969.895331	174119.575858	37.651085
1971.766745	174342.522161	37.656103
1974.090090	174550.834675	37.661120
1976.120694	174794.994295	37.666138
1978.097773	174988.521529	37.671156
1980.115369	175233.218676	37.676173
1982.305521	175448.382051	37.681191
1983.860997	175659.219800	37.686208
1986.096081	175864.838261	37.691226
1988.071833	176087.346308	37.696244
1990.393086	176300.527017	37.701261
1992.041324	176510.846999	37.706279
1993.704231	176754.302863	37.711296
1996.140746	176967.075471	37.716314
1998.011675	177167.112735	37.721332
2000.075247	177404.812579	37.726349
2002.076257	177614.257591	37.731367
2003.718358	177839.086300	37.736384
2006.144979	178052.842957	37.741402
2008.352747	178279.931378	37.746420
2010.182128	178482.886896	37.751437
2011.900519	178703.584879	37.756455
2013.976232	178906.452620	37.761472
2015.988352	179085.098850	37.766490
2017.427181	179298.599917	37.771508
2019.683508	179458.634820	37.776525
2021.415710	179710.838533	37.781543
2023.246850	179885.926334	37.786560
2025.419756	180108.462678	37.791578
2027.190604	180306.589632	37.796596
2029.290623	180521.514467	37.801613
2031.134868	180746.567689	37.806631
2033.150692	180934.939909	37.811648
2035.165529	181183.935555	37.816666
2036.511145	181384.165011	37.821684
2039.049457	181634.869209	37.826701
2041.438208	181853.548606	37.831719
2043.198643	182074.016306	37.836736
2045.446209	182302.122246	37.841754
2047.420122	182553.098926	37.846772
2049.763744	182762.032804	37.851789
2051.865090	182981.118737	37.856807
2053.766071	183229.560508	37.861824
2056.327877	183459.500523	37.866842
2058.093495	183678.655882	37.871860
2060.114981	183903.887654	37.876877
2062.458464	184143.242759	37.881895
2064.463938	184359.876455	37.886912
2066.643834	184602.140329	37.891930
2068.983117	184824.407923	37.896948
2071.259981	185042.410348	37.901965
2073.128521	185287.582340	37.906983
2075.431778	185499.301734	37.912000
2078.064759	185737.147515	37.917018
2080.233804	185939.601815	37.922036
2082.369828	186145.488359	37.927053
2084.506540	186400.775258	37.932071
2086.378360	186600.221526	37.937088
2088.897037	186812.521976	37.942106
2090.479421	187026.317021	37.947124
2093.061198	187254.496771	37.952141
2095.368041	187457.595812	37.957159
2097.481892	187673.822110	37.962176
2099.616088	187878.561981	37.967194
2101.689781	188099.123838	37.972212
2103.589282	188294.969162	37.977229
2106.206960	188507.731245	37.982247
2108.088581	188720.192285	37.987264
2110.273329	188928.253532	37.992282
2112.477249	189155.233571	37.997300
2114.784411	189334.115403	38.002317
2117.182740	189578.401371	38.007335
2119.085046	189746.080092	38.012352
2121.316999	189958.821109	38.017370
2123.014943	190165.543722	38.022388
2125.251544	190369.478739	38.027405
2127.832677	190539.958700	38.032423
2129.184053	190757.271927	38.037440
2131.360761	190905.253619	38.042458
2133.101838	191116.529416	38.047476
2135.495189	191258.107154	38.052493
2137.417887	191479.317893	38.057511
2139.361066	191661.451569	38.062528
2141.406480	191830.003257	38.067546
2143.203295	192057.861201	38.072564
2145.210756	192239.200020	38.077581
2147.458546	192441.086115	38.082599
2149.374359	192623.215047	38.087616
2151.416145	192842.940949	38.092634
2153.264929	193063.231471	38.097652
2155.496106	193277.434027	38.102669
2158.098660	193487.948924	38.107687
2159.934886	193705.008043	38.112704
2162.575617	193934.378025	38.117722
2164.486511	194152.937528	38.122740
2166.515094	194369.385235	38.127757
2168.746168	194590.941822	38.132775
2170.893672	194816.548558	38.137792
2173.250601	195029.926453	38.142810
2175.316356	195274.928301	38.147828
2177.716268	195486.803695	38.152845
2179.871554	195703.338578	38.157863
2182.004885	195938.877543	38.162880
2184.551302	196173.006744	38.167898
2186.786339	196397.756279	38.172916
2188.473229	196618.214986	38.177933
2191.206530	196852.038428	38.182951
2193.191309	197067.641525	38.187968
2195.364414	197314.235325	38.192986
2197.930498	197531.423534	38.198004
2200.196639	197754.232130	38.203021
2202.403379	197989.895744	38.208039
2204.181220	198198.644405	38.213056
2206.598520	198447.882932	38.218074
2208.978089	198656.601452	38.223092
2211.147088	198921.036439	38.228109
2213.704104	199125.045115	38.233127
2215.570840	199373.080663	38.238144
2218.162702	199594.791896	38.243162
2220.213237	199811.043148	38.248180
2222.591097	200066.946542	38.253197
2225.232441	200266.833732	38.258215
2227.320846	200511.196538	38.263232
2229.702098	200734.139007	38.268250
2231.984968	200944.912673	38.273268
2234.221093	201196.680571	38.278285
2236.527236	201383.525758	38.283303
2238.763406	201635.346442	38.288320
2241.210052	201824.303312	38.293338
2243.060678	202069.967431	38.298356
2245.793898	202272.665325	38.303373
2247.966513	202479.019697	38.308391
2249.980486	202677.276191	38.313408
2252.177267	202854.598240	38.318426
2254.236277	203067.560724	38.323444
2256.177003	203256.729632	38.328461
2258.120551	203435.439194	38.333479
2260.301503	203666.853823	38.338496
2262.408195	203880.027616	38.343514
2264.730319	204086.402282	38.348532
2266.660177	204292.903364	38.353549
2269.185727	204504.515222	38.358567
2270.927320	204747.809198	38.363584
2272.998414	204939.184480	38.368602
2275.303597	205183.977687	38.373620
2277.180724	205428.877883	38.378637
2279.867316	205649.113072	38.383655
2282.047621	205897.026454	38.388672
2284.549665	206136.613255	38.393690
2286.513602	206360.469312	38.398708
2288.569640	206609.306707	38.403725
2291.336223	206850.758630	38.408743
2293.432406	207106.180128	38.413760
2295.779489	207370.296740	38.418778
2298.133823	207609.785999	38.423796
2300.314725	207865.997078	38.428813
2302.387972	208105.304381	38.433831
2304.687129	208359.416896	38.438848
2307.029407	208630.509196	38.443866
2309.566270	208865.442491	38.448884
2311.951252	209162.948247	38.453901
2314.807498	209403.291763	38.458919
2317.121405	209654.716027	38.463936
2319.376538	209918.604429	38.468954
2322.087631	210164.750157	38.473972
2324.082418	210432.490536	38.478989
2326.381463	210675.529832	38.484007
2329.030569	210955.990830	38.489024
2331.454145	211189.973387	38.494042
2333.611983	211447.726472	38.499060
2336.199078	211709.563938	38.504077
2338.627054	211957.031109	38.509095
2340.699127	212225.871342	38.514112
2343.242823	212488.861476	38.519130
2345.750468	212728.638209	38.524148
2347.656796	212991.985345	38.529165
2350.339939	213250.221006	38.534183
2352.646413	213511.399330	38.539200
2355.144575	213763.331184	38.544218
2357.583284	214021.887947	38.549236
2359.651929	214283.932269	38.554253
2362.344312	214558.473100	38.559271
2364.302530	214788.467040	38.564288
2366.775603	215061.927463	38.569306
2369.250070	215306.543330	38.574324
2371.628248	215578.675115	38.579341
2374.166641	215841.285870	38.584359
2376.110418	216064.760627	38.589376
2377.961824	216297.937990	38.594394
2380.284470	216538.494168	38.599412
2382.413469	216778.866045	38.604429
2384.908231	217016.260616	38.609447
2387.457989	217267.042003	38.614464
2389.003598	217522.363740	38.619482
2391.526385	217779.220153	38.624500
2394.036366	218034.352803	38.629517
2396.448424	218294.517056	38.634535
2398.546366	218560.534421	38.639552
2400.523797	218831.485503	38.644570
2403.273962	219090.875359	38.649588
2405.415758	219380.415891	38.654605
2408.068297	219655.059409	38.659623
2410.325586	219933.740740	38.664640
2412.694152	220227.222828	38.669658
2415.083387	220505.669573	38.674676
2417.339814	220798.321012	38.679693
2420.083354	221072.041221	38.684711
2422.486987	221368.175967	38.689728
2425.020738	221667.427465	38.694746
2427.593286	221945.393432	38.699764
2429.800637	222306.509354	38.704781
2432.402526	222593.805553	38.709799
2434.904560	222890.273473	38.714816
2437.316720	223193.880040	38.719834
2440.170676	223485.583716	38.724852
2442.646877	223784.001862	38.729869
2445.104301	224080.379806	38.734887
2447.920342	224368.664428	38.739904
2450.472674	224663.620079	38.744922
2452.717745	224948.873664	38.749940
2454.881129	225250.661005	38.754957
2457.901031	225524.835660	38.759975
2460.149949	225826.294144	38.764992
2462.506818	226132.688816	38.770010
2465.587009	226416.227966	38.775028
2467.584110	226723.875457	38.780045
2470.407844	227006.873163	38.785063
2472.941343	227309.218910	38.790080
2475.292371	227600.496494	38.795098
2478.118051	227903.890106	38.800116
2480.671188	228184.826748	38.805133
2483.082550	228477.875519	38.810151
2485.543486	228770.130135	38.815168
2488.172651	229068.378091	38.820186
2490.776837	229357.132629	38.825204
2493.202783	229652.087798	38.830221
2495.695074	229939.566735	38.835239
2497.929214	230236.992347	38.840256
2500.319891	230536.298923	38.845274
2503.408167	230813.959132	38.850292
2505.847012	231130.301553	38.855309
2508.176565	231400.134432	38.860327
2510.553117	231659.979469	38.865344
2513.013186	231930.021794	38.870362
2515.558306	232184.228743	38.875380
2517.479736	232455.475433	38.880397
2520.032504	232723.194172	38.885415
2522.029491	232998.646465	38.890432
2524.696250	233273.536263	38.895450
2527.170579	233559.835611	38.900468
2529.423406	233855.390379	38.905485
2531.840832	234130.677694	38.910503
2534.285074	234421.581394	38.915520
2536.537714	234720.110380	38.920538
2539.302367	235014.419211	38.925556
2541.715972	235328.239687	38.930573
2544.270062	235624.031373	38.935591
2546.910306	235931.061816	38.940608
2549.144748	236242.526038	38.945626
2551.505386	236543.252958	38.950644
2554.028043	236874.484382	38.955661
2556.574734	237189.356190	38.960679
2559.665439	237515.953235	38.965696
2561.981081	237841.454929	38.970714
2564.451112	238162.843895	38.975732
2567.168591	238488.969645	38.980749
2570.172787	238813.425389	38.985767
2572.619150	239145.945845	38.990784
2575.252960	239464.874332	38.995802
2578.130231	239787.752862	39.000820
2580.551067	240122.972587	39.005837
2583.120624	240447.095512	39.010855
2585.956016	240762.515948	39.015872
2588.531093	241102.794006	39.020890
2591.159351	241431.888710	39.025908
2593.950881	241756.589681	39.030925
2596.609769	242085.655932	39.035943
2599.277048	242410.835546	39.040960
2601.531588	242750.102249	39.045978
2604.435434	243068.591304	39.050996
2606.951050	243419.604133	39.056013
2609.911632	243746.620388	39.061031
2612.539961	244071.912095	39.066048
2615.292138	244402.620686	39.071066
2617.796081	244738.551137	39.076084
2620.762932	245067.068359	39.081101
2623.300120	245397.762706	39.086119
2626.087904	245705.481383	39.091136
2628.628506	246039.910654	39.096154
2631.470002	246353.870857	39.101172
2633.915759	246689.129546	39.106189
2636.459397	247010.453845	39.111207
2639.445577	247337.830394	39.116224
2641.900042	247678.246426	39.121242
2644.747735	247997.010065	39.126260
2646.764069	248327.387389	39.131277
2649.677823	248640.553704	39.136295
2652.269147	248941.960181	39.141312
2654.125049	249253.847463	39.146330
2657.256646	249542.697520	39.151348
2659.650642	249858.437985	39.156365
2661.817294	250157.602568	39.161383
2664.544509	250460.285926	39.166400
2666.988863	250789.279815	39.171418
2669.522252	251102.155672	39.176436
2671.955994	251423.633647	39.181453
2674.741950	251750.111375	39.186471
2677.274386	252077.163322	39.191488
2679.675295	252422.373572	39.196506
2682.769507	252749.439407	39.201524
2685.467089	253100.827433	39.206541
2687.839736	253429.736126	39.211559
2690.453196	253780.021104	39.216576
2692.842621	254133.644483	39.221594
2695.624042	254490.813524	39.226612
2698.321900	254842.204788	39.231629
2701.102265	255203.033206	39.236647
2703.762283	255564.440188	39.241664
2706.490647	255927.996176	39.246682
2709.386846	256296.708284	39.251700
2712.066131	256662.940565	39.256717
2714.783989	257032.063229	39.261735
2717.732954	257402.369229	39.266752
2720.598021	257773.019362	39.271770
2723.502850	258128.523926	39.276788
2726.263735	258514.712665	39.281805
2729.185170	258880.884794	39.286823
2731.982737	259251.065299	39.291840
2734.508963	259619.282521	39.296858
2737.569124	259991.835780	39.301876
2740.398216	260360.793581	39.306893
2742.939126	260718.899759	39.311911
2746.310480	261107.866269	39.316928
2748.638948	261466.083267	39.321946
2751.732726	261841.986898	39.326964
2754.127417	262221.304092	39.331981
2757.022932	262589.593799	39.336999
2760.024576	262957.232061	39.342016
2762.624353	263333.037927	39.347034
2765.715144	263700.231061	39.352052
2768.512329	264079.105664	39.357069
2771.242333	264448.566788	39.362087
2774.154632	264820.158679	39.367104
2776.917078	265203.180653	39.372122
2779.955996	265557.580725	39.377140
2782.578975	265931.378758	39.382157
2785.150903	266302.568682	39.387175
2787.963009	266678.877734	39.392192
2790.840584	267048.013030	39.397210
2793.226938	267423.602605	39.402228
2796.239315	267799.423577	39.407245
2798.929126	268166.912827	39.412263
2801.285987	268512.379608	39.417280
2803.793684	268854.520287	39.422298
2806.848461	269216.516121	39.427316
2809.356740	269569.199473	39.432333
2812.051212	269923.174501	39.437351
2815.349649	270265.292331	39.442368
2817.303538	270638.234242	39.447386
2820.173885	270996.195652	39.452404
2823.083917	271357.300943	39.457421
2825.512443	271741.244035	39.462439
2828.150234	272108.438708	39.467456
2830.869937	272501.735215	39.472474
2833.741790	272882.280649	39.477492
2836.290673	273273.724571	39.482509
2838.890147	273680.555038	39.487527
2842.043029	274065.349415	39.492544
2844.813234	274465.167051	39.497562
2847.337052	274870.536286	39.502580
2850.913816	275267.177889	39.507597
2853.613570	275692.079949	39.512615
2856.486930	276089.899879	39.517632
2859.503425	276504.946050	39.522650
2862.478850	276909.126027	39.527668
2865.219894	277323.783864	39.532685
2867.946718	277742.559232	39.537703
2871.309306	278149.853134	39.542720
2874.075995	278584.143470	39.547738
2877.369066	278992.515093	39.552756
2880.577856	279413.576208	39.557773
2883.126448	279823.818232	39.562791
2886.401167	280245.960913	39.567808
2889.316820	280660.945691	39.572826
2892.128210	281071.297954	39.577844
2895.125456	281483.017753	39.582861
2897.893434	281900.514750	39.587879
2901.557604	282310.197817	39.592896
2904.247529	282727.884446	39.597914
2906.911425	283140.036987	39.602932
2909.941558	283550.657852	39.607949
2913.023245	283967.773450	39.612967
2915.921709	284385.959228	39.617984
2918.857014	284809.143221	39.623002
2921.793888	285218.786695	39.628020
2924.636012	285639.393513	39.633037
2927.396426	286064.966432	39.638055
2931.006710	286467.440000	39.643072
2933.537883	286893.759575	39.648090
2936.455690	287309.653026	39.653108
2939.595998	287728.457506	39.658125
2942.534110	288156.997392	39.663143
2945.392514	288566.801995	39.668160
2948.287640	288994.941120	39.673178
2951.350869	289399.504617	39.678196
2954.575204	289819.283737	39.683213
2957.330500	290237.967960	39.688231
2960.278329	290603.580211	39.693248
2962.922497	291000.485336	39.698266
2965.610569	291381.049020	39.703284
2968.637042	291769.306377	39.708301
2971.192573	292148.619769	39.713319
2974.180389	292539.295295	39.718336
2976.842115	292934.467236	39.723354
2979.759294	293325.914729	39.728372
2982.690213	293737.351070	39.733389
2985.321571	294150.002580	39.738407
2988.239934	294567.510537	39.743424
2991.079875	294981.194358	39.748442
2994.005467	295400.477697	39.753460
2997.041874	295831.707057	39.758477
2999.877251	296267.641298	39.763495
3002.867773	296703.473818	39.768512
3005.819672	297142.816942	39.773530
3009.098326	297599.533048	39.778548
3012.087929	298042.729190	39.783565
3014.844419	298495.359808	39.788583
3018.102648	298930.763710	39.793600
3021.170924	299394.773456	39.798618
3024.073760	299847.098000	39.803636
3027.337245	300306.222664	39.808653
3030.208662	300757.508251	39.813671
3033.378679	301210.650433	39.818688
3036.797264	301669.441883	39.823706
3039.789075	302133.481379	39.828724
3043.120363	302586.975078	39.833741
3046.158448	303050.674249	39.838759
3049.167599	303498.805744	39.843776
3052.148875	303964.847924	39.848794
3055.091745	304429.040413	39.853812
3058.381048	304895.386425	39.858829
3061.554425	305364.568695	39.863847
3064.940675	305820.253371	39.868864
3067.971711	306296.694118	39.873882
3070.808540	306759.828684	39.878900
3074.363450	307216.015302	39.883917
3077.117701	307692.316973	39.888935
3080.299840	308155.214091	39.893952
3083.769836	308621.391356	39.898970
3086.667187	309083.618887	39.903988
3089.996913	309547.630439	39.909005
3093.268823	310012.258942	39.914023
3096.749521	310467.149931	39.919040
3099.638816	310933.892714	39.924058
3102.940380	311391.576981	39.929076
3106.480708	311836.750564	39.934093
3109.272968	312288.517555	39.939111
3112.460757	312746.595309	39.944128
3115.621589	313202.389508	39.949146
3119.021898	313647.120777	39.954164
3122.106544	314099.494390	39.959181
3125.095502	314544.007618	39.964199
3128.195367	314950.352726	39.969216
3131.191050	315372.358200	39.974234
3133.825915	315782.583377	39.979252
3136.806611	316188.002701	39.984269
3139.416353	316608.260825	39.989287
3142.489025	317033.142577	39.994304
3145.619780	317463.550064	39.999322
3148.606971	317900.302428	40.004340
3151.723795	318336.371966	40.009357
3154.473321	318781.691559	40.014375
3157.984828	319222.545533	40.019392
3160.761990	319676.364677	40.024410
3163.786526	320132.326624	40.029428
3166.705315	320585.585541	40.034445
3169.544688	321060.823151	40.039463
3172.726889	321532.194483	40.044480
3175.929053	322022.353723	40.049498
3178.723723	322501.679566	40.054516
3182.357717	322989.377795	40.059533
3185.464169	323480.686799	40.064551
3188.582630	323968.968931	40.069568
3191.584384	324471.132908	40.074586
3195.120778	324976.815496	40.079604
3198.484971	325469.468855	40.084621
3201.684374	325983.629924	40.089639
3204.809234	326467.223509	40.094656
3208.236337	326975.348927	40.099674
3211.343967	327487.178515	40.104692
3214.688382	328001.049695	40.109709
3218.150829	328515.000393	40.114727
3221.246960	329022.047507	40.119744
3224.489286	329542.323986	40.124762
3227.778455	330054.488731	40.129780
3231.432952	330557.805859	40.134797
3234.261371	331080.752709	40.139815
3237.504149	331596.469288	40.144832
3241.087615	332109.335046	40.149850
3244.481387	332629.311893	40.154868
3247.917805	333143.793304	40.159885
3251.333004	333651.037352	40.164903
3254.755664	334167.824230	40.169920
3257.806011	334679.740006	40.174938
3261.530625	335197.360191	40.179956
3265.029641	335702.417626	40.184973
3268.129727	336213.399946	40.189991
3271.363454	336717.806167	40.195008
3274.975984	337229.512227	40.200026
3277.920244	337746.652216	40.205044
3281.259148	338245.215530	40.210061
3284.591376	338773.483553	40.215079
3288.097787	339270.819110	40.220096
3291.523923	339777.583414	40.225114
3294.579068	340288.617154	40.230132
3298.206706	340785.972460	40.235149
3301.145658	341286.885766	40.240167
3303.824606	341751.884210	40.245184
3307.231188	342230.550625	40.250202
3310.578940	342684.874162	40.255220
3313.272213	343178.067129	40.260237
3316.326535	343645.962302	40.265255
3319.514748	344140.236999	40.270272
3322.767348	344614.922806	40.275290
3325.528587	345104.103104	40.280308
3328.947098	345628.363371	40.285325
3332.086942	346120.445702	40.290343
3335.029292	346631.240435	40.295360
3338.914616	347152.417308	40.300378
3342.005842	347675.847516	40.305396
3345.457901	348191.396620	40.310413
3348.726667	348721.719693	40.315431
3351.882633	349240.987029	40.320448
3355.078440	349788.548908	40.325466
3358.803769	350337.062424	40.330484
3362.207175	350851.045894	40.335501
3365.227829	351419.486210	40.340519
3368.833598	351959.954980	40.345536
3372.244537	352509.409991	40.350554
3375.468839	353065.463463	40.355572
3379.078684	353617.160120	40.360589
3382.574114	354191.638664	40.365607
3385.808597	354740.209745	40.370624
3389.491079	355302.893603	40.375642
3392.643642	355874.107714	40.380660
3396.243222	356433.314674	40.385677
3399.900484	357003.268613	40.390695
3403.522368	357567.942096	40.395712
3406.915398	358118.329779	40.400730
3410.564960	358682.833884	40.405748
3414.218183	359252.001133	40.410765
3417.704447	359823.015583	40.415783
3421.276029	360382.385288	40.420800
3424.751100	360938.616528	40.425818
3428.042208	361498.550536	40.430836
3431.478274	362070.815145	40.435853
3435.164895	362632.399040	40.440871
3438.740199	363201.962966	40.445888
3442.375991	363759.201433	40.450906
3445.475089	364322.989649	40.455924
3448.993571	364876.045628	40.460941
3452.688636	365448.862051	40.465959
3455.861756	366020.281828	40.470976
3459.833209	366575.554854	40.475994
3463.225073	367162.075973	40.481012
3466.899526	367702.028655	40.486029
3470.308931	368267.291824	40.491047
3473.798311	368819.618514	40.496064
3477.429543	369386.557767	40.501082
3480.696570	369949.893090	40.506100
3484.483247	370512.276152	40.511117
3487.546735	371049.540122	40.516122
3490.610752	371559.403557	40.521127
3493.862503	372014.943608	40.526132
3496.650125	372416.366803	40.531136
3499.429078	372803.287369	40.536141
3501.940197	373100.142874	40.541146
3504.087985	373357.700273	40.546151
3506.175745	373592.192934	40.551156
3508.263469	373759.985084	40.556160
3509.845775	373879.981714	40.561165
3511.144048	373964.612956	40.566170
3512.583238	374044.363068	40.571175
3513.367519	374064.538755	40.576180
3514.413737	374071.038200	40.581184
3515.060726	374040.842659	40.586189
3515.778259	373987.588970	40.591194
3516.057816	373937.431589	40.596199
3516.699378	373863.788309	40.601204
3516.588122	373759.127416	40.606208
3517.247941	373662.866232	40.611213
3517.299289	373565.200137	40.616218
3517.530776	373424.641466	40.621223
3517.271501	373292.147614	40.626228
3517.404112	373170.937044	40.631232
3517.254438	373012.299458	40.636237
3516.945603	372875.487528	40.641242
3516.516546	372746.249516	40.646247
3517.056486	372571.322095	40.651252
3516.394759	372451.125368	40.656256
3516.538753	372276.742651	40.661261
3516.412495	372138.093276	40.666266
3515.928014	371991.995452	40.671271
3516.044678	371835.702630	40.676276
3515.307591	371694.197373	40.681280
3515.147834	371545.172007	40.686285
3515.251660	371418.415101	40.691290
3514.950383	371268.902342	40.696295
3514.549443	371120.396968	40.701300
3514.034942	370993.329497	40.706304
3513.881203	370851.576587	40.711309
3513.572521	370711.399548	40.716314
3513.121641	370606.428352	40.721319
3513.419531	370475.542098	40.726324
3513.003475	370351.840719	40.731328
3512.660922	370233.368095	40.736333
3512.606990	370106.148870	40.741338
3512.072318	369998.314657	40.746343
3511.788112	369887.235064	40.751348
3511.252326	369799.371423	40.756352
3511.511749	369689.579187	40.761357
3511.223912	369593.458572	40.766362
3510.803780	369493.593408	40.771367
3510.962470	369397.147366	40.776372
3510.668598	369311.432416	40.781376
3510.334778	369214.402355	40.786381
3510.563535	369140.358209	40.791386
3509.941525	369058.994172	40.796391
3510.199083	368965.889775	40.801396
3509.715818	368886.691425	40.806400
3509.282253	368797.105038	40.811405
3509.327964	368747.054832	40.816410
3509.426172	368672.292731	40.821415
3509.371796	368594.908717	40.826420
3509.057608	368521.076554	40.831424
3509.062466	368449.737981	40.836429
3508.807879	368392.738433	40.841434
3508.476520	368324.760200	40.846439
3508.485481	368265.479971	40.851444
3508.153204	368208.975855	40.856448
3508.236562	368154.822923	40.861453
3507.943531	368105.029064	40.866458
3507.817878	368051.824944	40.871463
3507.877105	367992.638168	40.876468
3507.815870	367946.445658	40.881472
3507.764657	367893.891066	40.886477
3507.498422	367843.202213	40.891482
3507.263436	367800.624312	40.896487
3507.400931	367755.824932	40.901492
3507.167749	367714.925827	40.906496
3507.210124	367671.820563	40.911501
3507.244022	367632.736425	40.916506
3506.935465	367583.784016	40.921511
3507.030471	367548.531882	40.926516
3506.753363	367504.866349	40.931520
3506.834250	367482.184749	40.936525
3507.031256	367441.115623	40.941530
3506.609681	367401.441785	40.946535
3506.719688	367359.215999	40.951540
3506.607365	367336.234119	40.956544
3506.773962	367293.973883	40.961549
3506.769995	367256.803560	40.966554
3506.438482	367218.056682	40.971559
3506.713607	367185.294563	40.976564
3506.297363	367164.014379	40.981568
3506.507140	367129.430710	40.986573
3506.273000	367098.809850	40.991578
3506.296322	367066.927042	40.996583
3506.365455	367034.324586	41.001588
3506.211772	367013.511672	41.006592
3506.080734	366989.896513	41.011597
3506.385356	366952.142867	41.016602
3506.170921	366926.327375	41.021607
3506.279810	366898.399927	41.026612
3506.208841	366868.847138	41.031616
3506.117254	366845.327437	41.036621
3506.441477	366815.686701	41.041626
3506.063281	366792.848337	41.046631
3506.376978	366753.948180	41.051636
3505.954290	366725.417706	41.056640
3506.091465	366705.678140	41.061645
3506.211670	366680.140360	41.066650
3506.270297	366651.482871	41.071655
3506.334113	366623.155296	41.076660
3506.322671	366592.269904	41.081664
3506.154160	366563.673706	41.086669
3506.102670	366540.529144	41.091674
3505.390382	366515.326405	41.096679
3505.779700	366484.733785	41.101684
3505.901852	366461.917931	41.106688
3505.581760	366441.792563	41.111693
3505.766744	366418.305247	41.116698
3505.899160	366403.883811	41.121703
3505.967033	366378.862985	41.126708
3505.749536	366361.469171	41.131712
3505.724266	366322.545893	41.136717
3505.638609	366308.947622	41.141722
3505.576493	366301.273776	41.146727
3505.798444	366262.107825	41.151732
3505.470905	366235.622860	41.156736
3505.696258	366219.660110	41.161741
3505.733307	366204.159646	41.166746
3505.616949	366182.882476	41.171751
3505.564635	366158.465709	41.176756
3505.231432	366146.865614	41.181760
3505.326399	366126.165639	41.186765
3505.369287	366116.312524	41.191770
3505.151007	366101.997313	41.196775
3505.323032	366077.977569	41.201780
3505.398583	366057.077088	41.206784
3505.353126	366054.412807	41.211789
3505.439278	366016.820123	41.216794
3505.183632	366018.158151	41.221799
3505.320577	365994.983522	41.226804
3505.422821	365981.533550	41.231808
3505.462030	365958.348908	41.236813
3505.249889	365944.185334	41.241818
3505.058466	365926.990773	41.246823
3505.365811	365903.382075	41.251828
3505.114334	365889.580902	41.256832
3505.135140	365882.937038	41.261837
3505.364006	365869.212587	41.266842
3505.113364	365852.256345	41.271847
3505.176601	365834.258205	41.276852
3504.993540	365818.258101	41.281856
3504.918385	365807.024215	41.286861
3504.958083	365796.331916	41.291866
3505.063839	365798.986745	41.296871
3505.286072	365778.928011	41.301876
3505.075052	365769.369387	41.306880
3505.235588	365760.235445	41.311885
3505.077165	365734.003325	41.316890
3504.881705	365718.514005	41.321895
3505.267049	365711.583504	41.326900
3505.112854	365704.153099	41.331904
3505.138558	365688.196278	41.336909
3504.897001	365663.147638	41.341914
3504.820943	365669.037040	41.346919
3505.126357	365642.680660	41.351924
3505.183632	365641.908345	41.356928
3504.650753	365629.729046	41.361933
3504.691317	365610.793007	41.366938
3504.875501	365611.832534	41.371943
3505.253771	365580.961174	41.376948
3505.015099	365571.076119	41.381952
3505.104394	365558.340475	41.386957
3504.963564	365550.195525	41.391962
3504.688344	365544.641573	41.396967
3504.881176	365521.864957	41.401972
3504.750381	365516.160956	41.406976
3504.656678	365493.327847	41.411981
3504.599828	365495.321432	41.416986
3504.570489	365485.250609	41.421991
3504.616382	365476.516379	41.426996
3504.315499	365485.901615	41.432000
3504.785232	365479.034069	41.437005
3504.884543	365455.534351	41.442010
3504.499164	365459.971528	41.447015
3504.988967	365455.467021	41.452020
3504.814183	365446.462351	41.457024
3504.447015	365441.584444	41.462029
3504.765233	365427.336872	41.467034
3504.910095	365415.482916	41.472039
3504.923103	365402.377639	41.477044
3504.879455	365386.889652	41.482048
3504.780530	365390.874463	41.487053
3505.020084	365376.079559	41.492058
3504.966008	365370.719617	41.497063
3505.010650	365356.947803	41.502068
3504.830854	365340.412705	41.507072
3504.743240	365334.192990	41.512077
3504.616768	365318.158321	41.517082
3504.573614	365317.045670	41.522087
3504.691433	365311.505890	41.527092
3504.612292	365301.900878	41.532096
3504.324206	365291.896356	41.537101
3504.556197	365297.380906	41.542106
3504.310415	365280.627228	41.547111
3504.627128	365259.204835	41.552116
3504.782426	365287.625910	41.557120
3504.694734	365269.549630	41.562125
3504.693334	365253.698713	41.567130
3504.475168	365253.707788	41.572135
3504.800982	365229.841387	41.577140
3504.345058	365225.842558	41.582144
3504.666706	365224.672240	41.587149
3504.754134	365217.915974	41.592154
3504.358644	365208.055628	41.597159
3504.824933	365193.173937	41.602164
3504.857577	365190.649918	41.607168
3505.006017	365184.087549	41.612173
3504.938747	365170.358812	41.617178
3504.894833	365152.122906	41.622183
3505.045658	365133.754436	41.627188
3504.923639	365124.207050	41.632192
3504.912295	365112.708472	41.637197
3505.198593	365097.041013	41.642202
3505.248317	365087.542802	41.647207
3505.300813	365065.653217	41.652212
3505.323954	365057.991126	41.657216
3504.869681	365028.803043	41.662221
3504.577478	365028.187735	41.667226
3504.368885	365013.692544	41.672231
3504.478890	365001.716774	41.677236
3504.523944	364996.773657	41.682240
3504.583257	364997.324068	41.687245
3505.104608	364981.568527	41.692250
3504.883952	364975.268020	41.697255
3504.878401	364968.857179	41.702260
3504.882045	364957.966835	41.707264
3504.982568	364940.191438	41.712269
3504.911782	364935.571947	41.717274
3504.549091	364916.979242	41.722279
3504.779654	364905.722250	41.727284
3504.664551	364886.327090	41.732288
3504.317588	364905.032049	41.737293
3504.869619	364862.326954	41.742298
3504.624339	364869.388167	41.747303
3504.526158	364871.617304	41.752308
3504.421325	364865.018594	41.757312
3504.496688	364847.552460	41.762317
3504.611700	364849.417132	41.767322
3504.510546	364839.764615	41.772327
3504.894372	364825.048500	41.777332
3504.511554	364821.826829	41.782336
3504.295781	364814.431456	41.787341
3504.325871	364796.870685	41.792346
3504.598475	364791.866133	41.797351
3504.333584	364792.722230	41.802356
3504.447111	364794.943349	41.807360
3504.499132	364771.883294	41.812365
3504.652601	364764.633094	41.817370
3504.603187	364783.087519	41.822375
3504.697271	364759.944479	41.827380
3504.504987	364750.357235	41.832384
3504.649741	364758.832538	41.837389
3504.733099	364748.158536	41.842394
3504.268372	364739.225001	41.847399
3504.144633	364733.545230	41.852404
3504.325417	364737.842094	41.857408
3504.601151	364724.313438	41.862413
3504.579584	364711.289759	41.867418
3504.314484	364705.530555	41.872423
3504.752174	364698.057311	41.877428
3504.886920	364688.927232	41.882432
3504.994054	364675.628762	41.887437
3504.696001	364665.600234	41.892442
3504.492800	364659.322368	41.897447
3504.550375	364644.861316	41.902452
3504.691270	364625.781790	41.907456
3504.697555	364626.645912	41.912461
3504.571947	364616.233904	41.917466
3504.693589	364619.395163	41.922471
3504.640090	364598.667073	41.927476
3504.493688	364595.815113	41.932480
3504.538546	364584.867278	41.937485
3504.493223	364563.094690	41.942490
3504.565250	364571.479749	41.947495
3504.679954	364563.726771	41.952500
3504.157014	364564.852657	41.957504
3504.605460	364550.533338	41.962509
3504.800002	364547.220382	41.967514
3504.562512	364534.917764	41.972519
3504.757243	364530.688804	41.977524
3504.747691	364522.777355	41.982528
3504.674481	364509.227464	41.987533
3504.756138	364491.047775	41.992538
3504.380969	364488.842620	41.997543
3504.257293	364475.504247	42.002548
3504.415013	364458.661039	42.007552
3504.447617	364451.786107	42.012557
3504.432816	364469.471875	42.017562
3504.178196	364464.219859	42.022567
3504.669301	364439.461831	42.027572
3504.537122	364445.309374	42.032576
3504.691718	364441.392075	42.037581
3504.716408	364430.752716	42.042586
3504.636015	364429.976699	42.047591
3505.026089	364413.987278	42.052596
3504.905496	364399.757863	42.057600
3504.731259	364380.473611	42.062605
3505.030028	364352.209254	42.067610
3504.515307	364356.005443	42.072615
3504.586396	364343.755771	42.077620
3504.819900	364324.890475	42.082624
3504.508477	364327.560447	42.087629
3504.767598	364307.062690	42.092634
3504.288532	364297.800566	42.097639
3504.774360	364292.380597	42.102644
3504.623825	364290.750575	42.107648
3504.381350	364274.657544	42.112653
3504.682488	364253.517026	42.117658
3504.423000	364263.201294	42.122663
3504.316620	364243.193831	42.127668
3504.707243	364229.519650	42.132672
3504.370123	364233.313219	42.137677
3504.418192	364233.254764	42.142682
3504.323375	364232.277473	42.147687
3504.416675	364214.731932	42.152692
3504.036316	364217.870797	42.157696
3504.195699	364217.413088	42.162701
3504.496297	364210.953747	42.167706
3504.091133	364200.000625	42.172711
3504.178882	364197.798612	42.177716
3504.022510	364203.751786	42.182720
3504.280131	364194.347746	42.187725
3504.488478	364197.215446	42.192730
3504.287521	364191.318819	42.197735
3504.529134	364171.510754	42.202740
3504.430910	364172.544068	42.207744
3504.107209	364191.296529	42.212749
3504.643362	364170.754920	42.217754
3504.274810	364166.716742	42.222759
3504.381835	364154.842997	42.227764
3504.357476	364154.872323	42.232768
3504.502443	364152.941146	42.237773
3504.216668	364148.889882	42.242778
3504.128634	364140.787222	42.247783
3504.351947	364136.731815	42.252788
3504.289098	364148.445981	42.257792
3504.009387	364154.113332	42.262797
3504.319370	364136.584396	42.267802
3504.036139	364119.225557	42.272807
3504.300795	364110.507374	42.277812
3504.299125	364138.546872	42.282816
3504.501954	364102.511688	42.287821
3504.393811	364114.792789	42.292826
3504.411476	364085.809386	42.297831
3504.534490	364095.713109	42.302836
3504.360411	364099.506360	42.307840
3504.110829	364075.908422	42.312845
3504.222497	364072.125097	42.317850
3504.125592	364053.515470	42.322855
3504.194821	364064.878008	42.327860
3504.040372	364066.658087	42.332864
3504.289278	364072.979761	42.337869
3504.653654	364068.825718	42.342874
3504.342123	364064.727630	42.347879
3504.693768	364044.571346	42.352884
3504.643189	364049.668166	42.357888
3504.737963	364019.807437	42.362893
3504.756726	364004.283672	42.367898
3504.429414	364009.602348	42.372903
3504.923118	363981.535945	42.377908
3504.605056	363992.374509	42.382912
3504.515333	363985.569733	42.387917
3504.374852	363947.909392	42.392922
3504.275095	363957.568475	42.397927
3504.254962	363946.783426	42.402932
3504.542362	363957.170074	42.407936
3504.492467	363942.954787	42.412941
3504.456593	363929.551487	42.417946
3504.286743	363935.761266	42.422951
3504.472474	363925.630659	42.427956
3504.018857	363923.183436	42.432960
3503.925829	363899.331664	42.437965
3504.261303	363892.332440	42.442970
3503.907132	363901.166654	42.447975
3504.244383	363892.106181	42.452980
3504.449230	363906.576938	42.457984
3504.069694	363897.756993	42.462989
3504.567762	363876.941389	42.467994
3503.874246	363886.338129	42.472999
3504.188944	363881.199604	42.478004
3504.281759	363869.429808	42.483008
3504.198355	363898.423802	42.488013
3504.356581	363885.854905	42.493018
3503.949551	363861.976417	42.498023
3504.186591	363866.111805	42.503028
3504.441578	363857.547767	42.508032
3504.766251	363859.353893	42.513037
3504.450293	363849.989563	42.518042
3504.462717	363845.331365	42.523047
3504.549514	363819.364711	42.528052
3504.454307	363838.513745	42.533056
3504.429742	363828.772576	42.538061
3504.377343	363805.117884	42.543066
3503.925300	363806.588798	42.548071
3504.322104	363804.974015	42.553076
3504.435917	363806.762587	42.558080
3504.150100	363801.515426	42.563085
3504.323049	363781.132834	42.568090
3504.320245	363782.532734	42.573095
3504.457986	363765.081773	42.578100
3504.027499	363797.540208	42.583104
3503.996674	363772.075558	42.588109
3504.578185	363756.539086	42.593114
3504.256778	363756.691701	42.598119
3504.560621	363755.396940	42.603124
3504.681287	363757.515204	42.608128
3504.193139	363739.959618	42.613133
3504.535561	363736.928557	42.618138
3504.481807	363736.122873	42.623143
3504.091344	363721.172584	42.628148
3504.108643	363727.403696	42.633152
3504.517295	363714.769723	42.638157
3504.638865	363710.475920	42.643162
3504.250925	363699.265515	42.648167
3504.101948	363687.712003	42.653172
3504.236228	363691.889095	42.658176
3504.209215	363685.227026	42.663181
3504.487626	363674.572830	42.668186
3504.005700	363684.139717	42.673191
3504.293072	363690.786137	42.678196
3504.070548	363674.715187	42.683200
3503.934767	363649.470614	42.688205
3504.389612	363646.879772	42.693210
3504.171335	363665.335894	42.698215
3504.533444	363650.750059	42.703220
3504.171615	363671.188073	42.708224
3504.230587	363662.171545	42.713229
3504.621825	363634.960786	42.718234
3504.278505	363640.587366	42.723239
3504.413268	363633.950605	42.728244
3504.412867	363615.325547	42.733248
3503.971955	363619.466348	42.738253
3504.170275	363602.234747	42.743258
3503.935345	363606.851873	42.748263
3504.295256	363600.637513	42.753268
3504.509841	363600.985287	42.758272
3504.314352	363598.777130	42.763277
3503.903181	363585.585721	42.768282
3503.967419	363588.756126	42.773287
3504.039367	363582.765392	42.778292
3504.013294	363582.871322	42.783296
3504.118031	363585.806327	42.788301
3504.418368	363589.193853	42.793306
3504.234384	363596.652678	42.798311
3504.257100	363568.838585	42.803316
3504.203228	363568.211027	42.808321
3503.995910	363568.803603	42.813325
3504.211495	363563.222714	42.818330
3504.093085	363567.745092	42.823335
3504.312284	363564.250059	42.828340
3504.357132	363549.536233	42.833345
3504.168372	363549.108106	42.838349
3504.493746	363534.095489	42.843354
3504.308237	363543.233885	42.848359
3504.146869	363528.399985	42.853364
3504.149398	363531.173040	42.858369
3504.226282	363515.181927	42.863373
3504.729592	363510.369765	42.868378
3504.487388	363512.774400	42.873383
3504.488686	363499.136101	42.878388
3504.589691	363489.451344	42.883393
3504.434564	363487.847463	42.888397
3504.478751	363469.724184	42.893402
3504.279287	363464.717778	42.898407
3504.129311	363445.225746	42.903412
3504.280048	363449.044038	42.908417
3504.001825	363453.718911	42.913421
3504.519442	363451.805131	42.918426
3504.056610	363443.787039	42.923431
3504.072691	363423.505419	42.928436
3504.354669	363425.089313	42.933441
3504.061046	363428.519852	42.938445
3504.687357	363419.464483	42.943450
3504.347561	363412.190266	42.948455
3504.102428	363395.715684	42.953460
3504.467271	363388.330077	42.958465
3504.521789	363394.886127	42.963469
3504.718093	363388.901155	42.968474
3504.346385	363381.453867	42.973479
3504.501988	363357.104515	42.978484
3504.444083	363373.932409	42.983489
3504.086334	363358.569721	42.988493
3504.234674	363338.292602	42.993498
3504.165461	363335.072141	42.998503
3504.309511	363333.268297	43.003508
3504.334118	363341.661076	43.008513
3504.459067	363339.809363	43.013517
3505.063437	363319.256594	43.018522
3504.468085	363312.887866	43.023527
3504.360660	363305.805900	43.028532
3504.553812	363287.582669	43.033537
3503.936446	363292.514723	43.038541
3504.373457	363278.502152	43.043546
3504.140572	363280.650880	43.048551
3504.624466	363275.638209	43.053556
3504.487812	363262.428758	43.058561
3504.267472	363243.049541	43.063565
3504.716724	363248.932549	43.068570
3504.500863	363250.493366	43.073575
3504.531607	363218.708468	43.078580
3504.400104	363222.902172	43.083585
3504.171713	363219.503309	43.088589
3504.369797	363210.820925	43.093594
3504.132694	363195.413669	43.098599
3504.340365	363183.549210	43.103604
3504.202542	363195.428135	43.108609
3504.310139	363174.495829	43.113613
3504.250613	363186.845824	43.118618
3503.937353	363163.944486	43.123623
3504.081378	363152.726191	43.128628
3504.102063	363157.608289	43.133633
3504.027165	363164.261161	43.138637
3504.022374	363156.068837	43.143642
3503.804152	363163.100588	43.148647
3504.071254	363162.015175	43.153652
3504.026367	363164.159636	43.158657
3504.063117	363164.866303	43.163661
3504.303000	363158.390969	43.168666
3504.046980	363148.330022	43.173671
3504.088820	363143.845214	43.178676
3504.438081	363140.533146	43.183681
3504.392754	363146.494346	43.188685
3504.418243	363146.617571	43.193690
3504.190311	363128.028284	43.198695
3504.132280	363116.689254	43.203700
3504.192589	363128.333321	43.208705
3504.212931	363118.610349	43.213709
3504.186552	363119.810440	43.218714
3504.015822	363122.941686	43.223719
3504.015921	363104.189121	43.228724
3503.919168	363093.543208	43.233729
3503.728722	363088.738891	43.238733
3503.931654	363089.724624	43.243738
3503.955463	363100.585688	43.248743
3504.247858	363096.468381	43.253748
3504.403334	363089.955491	43.258753
3504.223227	363083.979093	43.263757
3504.714604	363079.601331	43.268762
3504.399142	363068.226649	43.273767
3504.142568	363077.910704	43.278772
3504.367068	363061.972434	43.283777
3504.276727	363052.953946	43.288781
3504.080822	363037.514680	43.293786
3504.273780	363039.748771	43.298791
3504.150917	363027.071408	43.303796
3504.042049	363041.083136	43.308801
3504.138286	363032.951153	43.313805
3504.168897	363044.218267	43.318810
3504.161929	363043.735955	43.323815
3504.343025	363016.049163	43.328820
3504.449901	363009.442166	43.333825
3504.305304	363008.269161	43.338829
3504.245878	363015.428501	43.343834
3503.741724	363006.373639	43.348839
3504.268906	363004.458329	43.353844
3504.285729	362998.807014	43.358849
3503.966121	362985.524626	43.363853
3504.398837	362971.716199	43.368858
3504.152794	362984.350176	43.373863
3504.148730	362987.658642	43.378868
3504.355085	362992.282405	43.383873
3504.208094	362966.377675	43.388877
3504.455361	362955.015790	43.393882
3504.068459	362959.249890	43.398887
3504.381249	362955.740016	43.403892
3504.164076	362951.728692	43.408897
3503.899615	362931.771095	43.413901
3504.221776	362911.542647	43.418906
3504.125345	362918.682406	43.423911
3504.117917	362933.390579	43.428916
3504.711167	362921.490548	43.433921
3504.340922	362903.636116	43.438925
3504.141195	362900.919703	43.443930
3503.902664	362893.349506	43.448935
3504.201535	362883.200788	43.453940
3503.966545	362884.128526	43.458945
3504.058095	362891.289463	43.463949
3504.168373	362891.501064	43.468954
3503.675374	362908.397903	43.473959
3503.946321	362907.159209	43.478964
3504.069817	362898.056000	43.483969
3504.031534	362908.468921	43.488973
3504.200881	362886.610720	43.493978
3503.800253	362890.846995	43.498983
3504.122368	362872.577772	43.503988
3504.034726	362884.677845	43.508993
3503.568138	362881.723725	43.513997
3504.399810	362878.488048	43.519002
3504.151104	362893.895933	43.524007
3504.541247	362882.206111	43.529012
3504.470056	362870.640100	43.534017
3504.145011	362859.292326	43.539021
3504.286370	362862.196143	43.544026
3503.870138	362868.648568	43.549031
3504.512986	362864.781179	43.554036
3504.497906	362849.491379	43.559041
3504.294284	362838.811411	43.564045
3504.242427	362832.611150	43.569050
3504.441733	362841.612520	43.574055
3504.465521	362823.517658	43.579060
3504.316502	362800.055841	43.584065
3504.430021	362803.549290	43.589069
3504.515572	362793.332493	43.594074
3504.127462	362801.917833	43.599079
3503.942115	362803.880957	43.604084
3504.437105	362774.490501	43.609089
3503.790562	362773.218723	43.614093
3504.206651	362765.697694	43.619098
3504.084261	362778.770185	43.624103
3504.191934	362769.694896	43.629108
3503.914028	362777.041476	43.634113
3503.986717	362783.162180	43.639117
3504.273607	362759.656881	43.644122
3504.346174	362755.879630	43.649127
3504.174140	362743.973303	43.654132
3504.211624	362741.677388	43.659137
3503.790749	362748.232342	43.664141
3504.313510	362753.645789	43.669146
3504.274957	362743.041484	43.674151
3504.261473	362725.334147	43.679156
3504.242332	362723.759633	43.684161
3504.159087	362713.442278	43.689165
3504.200991	362712.010783	43.694170
3503.874585	362735.496971	43.699175
3504.197770	362724.428366	43.704180
3504.174786	362706.620744	43.709185
3503.975231	362694.820533	43.714189
3504.142721	362690.901049	43.719194
3503.629098	362693.043293	43.724199
3504.100092	362693.706768	43.729204
3504.153889	362687.489787	43.734209
3504.053447	362695.037330	43.739213
3504.057495	362694.247935	43.744218
3503.978676	362708.102344	43.749223
3504.101470	362696.912741	43.754228
3504.051990	362677.658949	43.759233
3503.928180	362680.910030	43.764237
3504.236335	362676.230412	43.769242
3504.246715	362684.752782	43.774247
3503.954207	362680.193559	43.779252
3504.266652	362667.752623	43.784257
3503.840655	362690.262233	43.789261
3504.124605	362687.596574	43.794266
3504.020053	362665.450785	43.799271
3503.848925	362649.651248	43.804276
3504.044024	362649.900331	43.809281
3503.821146	362653.904972	43.814285
3504.032095	362647.154249	43.819290
3503.911173	362651.702557	43.824295
3504.203846	362650.943872	43.829300
3504.418710	362659.688370	43.834305
3504.028865	362658.299677	43.839309
3504.516561	362648.782622	43.844314
3504.057221	362638.626480	43.849319
3504.100329	362630.960832	43.854324
3504.053065	362627.253402	43.859329
3504.217478	362631.145934	43.864333
3504.385618	362635.063322	43.869338
3504.148243	362637.085566	43.874343
3504.142408	362606.527380	43.879348
3504.248244	362595.823884	43.884353
3503.860015	362618.454781	43.889357
3504.192044	362605.959844	43.894362
3504.188709	362604.382828	43.899367
3503.937490	362598.392164	43.904372
3504.197346	362601.353600	43.909377
3503.915141	362596.309289	43.914381
3504.064207	362585.013728	43.919386
3504.105913	362572.539230	43.924391
3504.332750	362558.101661	43.929396
3504.231092	362581.984960	43.934401
3504.227707	362580.484285	43.939405
3504.271940	362573.632681	43.944410
3504.186527	362561.559946	43.949415
3503.723931	362548.147368	43.954420
3504.227113	362547.304516	43.959425
3504.357554	362537.131457	43.964429
3504.054045	362538.528040	43.969434
3503.867212	362544.002790	43.974439
3504.317613	362551.921287	43.979444
3504.461819	362532.865821	43.984449
3504.409147	362526.640204	43.989453
3504.681754	362515.325097	43.994458
3504.468026	362519.328303	43.999463
3504.478711	362497.138773	44.004468
3504.150466	362486.860097	44.009473
3503.887323	362480.031623	44.014477
3504.299799	362475.462719	44.019482
3504.014487	362475.126179	44.024487
3504.356474	362482.832822	44.029492
3504.458635	362466.353902	44.034497
3504.153250	362461.771248	44.039501
3504.298137	362453.656919	44.044506
3504.315342	362466.961879	44.049511
3504.475008	362452.840234	44.054516
3504.563403	362432.012411	44.059521
3504.207670	362429.982197	44.064525
3504.342866	362417.645548	44.069530
3504.107133	362428.522351	44.074535
3504.419856	362406.208700	44.079540
3504.456773	362385.236324	44.084545
3503.799629	362400.658045	44.089549
3504.218463	362387.716766	44.094554
3503.815240	362394.625207	44.099559
3504.034734	362386.270069	44.104564
3503.770688	362388.372875	44.109569
3504.206207	362408.125613	44.114573
3504.013346	362395.637257	44.119578
3504.267446	362379.592297	44.124583
3504.135620	362363.481112	44.129588
3504.153941	362363.122019	44.134593
3503.999757	362362.612081	44.139597
3504.260248	362367.761692	44.144602
3504.278593	362374.298158	44.149607
3504.187076	362356.348568	44.154612
3504.131115	362341.243179	44.159617
3504.254527	362342.979400	44.164621
3504.229794	362330.973348	44.169626
3504.152168	362343.021088	44.174631
3503.891933	362336.828256	44.179636
3503.896884	362346.013113	44.184641
3503.987324	362341.622326	44.189645
3504.234364	362331.863355	44.194650
3504.179456	362315.790885	44.199655
3504.071451	362314.001401	44.204660
3504.026356	362309.530256	44.209665
3503.789405	362310.280201	44.214669
3504.403778	362309.852332	44.219674
3504.414978	362320.283007	44.224679
3504.383961	362293.850673	44.229684
3504.376176	362282.630723	44.234689
3504.063491	362274.614139	44.239693
3504.391208	362278.735335	44.244698
3504.332571	362273.986434	44.249703
3504.190619	362267.545891	44.254708
3504.236679	362247.844255	44.259713
3504.068390	362249.168582	44.264717
3504.318782	362246.304643	44.269722
3504.114455	362244.886612	44.274727
3504.086220	362239.445887	44.279732
3504.194332	362245.459282	44.284737
3504.124628	362232.900525	44.289741
3504.175038	362214.801221	44.294746
3504.106739	362214.608489	44.299751
3504.132458	362223.204853	44.304756
3504.188642	362218.412350	44.309761
3503.851158	362225.284979	44.314765
3504.125627	362219.338393	44.319770
3503.875168	362200.854079	44.324775
3503.778498	362187.561668	44.329780
3503.875050	362171.388872	44.334785
3503.717076	362189.225364	44.339789
3503.950835	362190.766033	44.344794
3503.769679	362195.832807	44.349799
3504.308288	362194.246444	44.354804
3504.269979	362192.725833	44.359809
3503.716828	362194.263667	44.364813
3504.125544	362192.239828	44.369818
3503.918971	362193.595652	44.374823
3504.050531	362196.221165	44.379828
3504.464764	362203.483869	44.384833
3503.932190	362200.311131	44.389837
3504.017834	362172.308144	44.394842
3504.201955	362172.177291	44.399847
3504.165430	362156.610761	44.404852
3504.446658	362185.166506	44.409857
3504.041184	362174.060284	44.414861
3504.059374	362162.556304	44.419866
3503.956382	362151.911162	44.424871
3504.027178	362146.403882	44.429876
3504.099434	362133.644544	44.434881
3504.100017	362144.407721	44.439885
3503.896067	362138.638531	44.444890
3504.061306	362151.360389	44.449895
3504.012405	362148.874541	44.454900
3503.899254	362139.757702	44.459905
3504.017968	362147.983149	44.464909
3503.939982	362142.931953	44.469914
3503.883359	362162.228245	44.474919
3503.517997	362138.240505	44.479924
3503.911401	362134.208928	44.484929
3504.107605	362144.126942	44.489933
3503.855060	362121.240940	44.494938
3503.564150	362124.976485	44.499943
3503.775364	362118.454650	44.504948
3503.965337	362118.908107	44.509953
3503.630166	362131.098392	44.514957
3503.880997	362135.129975	44.519962
3503.453144	362137.767586	44.524967
3503.693735	362132.106239	44.529972
3504.059801	362141.768397	44.534977
3503.865641	362137.549805	44.539981
3503.919469	362145.149384	44.544986
3504.055190	362142.100006	44.549991
3504.336808	362129.104011	44.554996
3504.447759	362152.241460	44.560001
3504.250063	362152.120072	44.565005
3504.280439	362123.413333	44.570010
3504.043019	362100.295925	44.575015
3503.936880	362119.625507	44.580020
3504.147647	362099.287093	44.585025
3504.223541	362103.702563	44.590029
3504.335161	362110.071651	44.595034
3504.210454	362115.943751	44.600039
3504.072663	362093.115930	44.605044
3503.877482	362087.294458	44.610049
3503.774286	362071.916553	44.615053
3504.150806	362080.864611	44.620058
3504.165119	362090.989504	44.625063
3504.130128	362096.414858	44.630068
3504.262629	362089.422006	44.635073
3504.043553	362083.884205	44.640077
3504.248031	362076.854528	44.645082
3504.011838	362070.785086	44.650087
3504.291922	362050.028573	44.655092
3504.049798	362047.904049	44.660097
3503.971937	362060.308129	44.665101
3504.183433	362064.702167	44.670106
3504.245756	362060.061348	44.675111
3504.073933	362059.808645	44.680116
3504.064933	362043.499819	44.685121
3504.173586	362029.157105	44.690125
3504.296885	362030.435345	44.695130
3503.999968	362039.489864	44.700135
3504.100846	362039.448504	44.705140
3504.393214	362031.590685	44.710145
3503.902948	362021.032177	44.715149
3504.111851	362006.037482	44.720154
3504.180753	362000.250589	44.725159
3504.015233	362000.531236	44.730164
3504.115640	361998.683350	44.735169
3504.220538	362005.155295	44.740173
3504.206725	361994.877697	44.745178
3503.832604	362004.326103	44.750183
3504.070686	362006.247771	44.755188
3504.099757	361981.408804	44.760193
3503.847923	361978.242562	44.765197
3504.066676	361976.681309	44.770202
3504.155741	361979.415332	44.775207
3504.010073	361979.234829	44.780212
3504.084548	361976.347792	44.785217
3503.854349	361988.292515	44.790221
3504.286530	361974.661996	44.795226
3504.106338	361982.680271	44.800231
3504.132280	361971.404025	44.805236
3504.365049	361947.347083	44.810241
3504.034690	361942.793771	44.815245
3504.296773	361946.162019	44.820250
3504.178110	361948.547203	44.825255
3504.240388	361948.384719	44.830260
3504.140201	361933.489751	44.835265
3504.022556	361927.401551	44.840269
3503.724034	361916.202026	44.845274
3503.881813	361921.953161	44.850279
3503.778200	361922.961931	44.855284
3503.839178	361917.837853	44.860289
3503.981007	361922.548258	44.865293
3503.773951	361915.812617	44.870298
3503.903211	361924.443558	44.875303
3503.754229	361924.874262	44.880308
3504.156586	361928.703794	44.885313
3504.077727	361935.688254	44.890317
3504.170759	361931.780477	44.895322
3503.733570	361934.699470	44.900327
3504.153518	361926.999583	44.905332
3504.132533	361897.970039	44.910337
3504.074063	361909.353288	44.915341
3504.203212	361895.465306	44.920346
3504.297534	361900.946577	44.925351
3504.058508	361903.579796	44.930356
3504.035429	361898.519894	44.935361
3503.851189	361904.477766	44.940365
3503.838529	361896.235575	44.945370
3503.930757	361909.299827	44.950375
3503.651760	361896.875845	44.955380
3504.272534	361883.597164	44.960385
3504.134929	361884.433192	44.965389
3504.197333	361872.107908	44.970394
3504.393388	361868.387401	44.975399
3504.075275	361869.226518	44.980404
3504.428279	361868.432839	44.985409
3504.326332	361855.573737	44.990413
3504.225263	361843.274286	44.995418
3504.421504	361839.273851	45.000423
3504.117467	361832.019179	45.005428
3504.201251	361838.341814	45.010433
3503.889017	361849.179952	45.015437
3504.132697	361814.892262	45.020442
3504.116758	361804.055164	45.025447
3504.301003	361802.473915	45.030452
3504.395704	361797.929733	45.035457
3504.122001	361817.184145	45.040461
3503.829028	361812.701246	45.045466
3504.091839	361811.183913	45.050471
3503.882095	361795.288412	45.055476
3503.958488	361778.151751	45.060481
3503.855790	361776.514078	45.065485
3504.027098	361763.026516	45.070490
3504.036036	361781.294792	45.075495
3503.820607	361775.272919	45.080500
3503.985093	361775.272395	45.085505
3503.730943	361778.137019	45.090509
3503.980022	361774.738910	45.095514
3504.110183	361780.112749	45.100519
3503.873303	361788.318134	45.105524
3504.095201	361781.361996	45.110529
3503.810900	361795.249155	45.115533
3504.036379	361790.429847	45.120538
3503.877749	361787.834099	45.125543
3503.939779	361779.223848	45.130548
3504.190521	361751.881535	45.135553
3503.887631	361763.685134	45.140557
3504.343816	361750.865003	45.145562
3504.331148	361754.607484	45.150567
3503.992470	361760.767903	45.155572
3504.217424	361757.373607	45.160577
3504.112186	361770.927125	45.165581
3504.133641	361748.175746	45.170586
3504.196530	361732.593360	45.175591
3503.870670	361743.281006	45.180596
3504.413023	361725.307311	45.185601
3504.081230	361726.708388	45.190605
3504.451341	361725.199536	45.195610
3504.256152	361720.650281	45.200615
3503.779861	361707.824868	45.205620
3504.145770	361675.502484	45.210625
3504.196121	361688.369854	45.215629
3504.098287	361693.856079	45.220634
3504.052655	361692.718288	45.225639
3503.768874	361684.391691	45.230644
3504.275211	361705.863807	45.235649
3504.110241	361684.515909	45.240653
3503.955624	361662.606570	45.245658
3503.958447	361676.906391	45.250663
3503.634696	361656.041595	45.255668
3504.058970	361656.279902	45.260673
3503.863098	361665.369411	45.265677
3504.006930	361668.934488	45.270682
3503.898637	361670.732806	45.275687
3504.111634	361669.070671	45.280692
3503.883554	361661.422287	45.285697
3503.848981	361680.079159	45.290701
3504.320239	361662.065789	45.295706
3504.195309	361668.904899	45.300711
3504.124161	361658.534510	45.305716
3504.091008	361646.682287	45.310721
3503.910005	361645.845791	45.315725
3503.949435	361635.559699	45.320730
3503.983646	361635.070862	45.325735
3503.695036	361632.800995	45.330740
3504.241157	361643.147262	45.335745
3503.797987	361650.087571	45.340749
3503.699257	361633.614672	45.345754
3503.919132	361641.696990	45.350759
3503.852231	361638.755945	45.355764
3503.528861	361645.041185	45.360769
3503.839915	361647.307567	45.365773
3504.231031	361647.372999	45.370778
3503.948392	361656.221772	45.375783
3503.866728	361656.743618	45.380788
3503.930595	361649.761550	45.385793
3503.866579	361632.367133	45.390797
3503.899999	361617.323719	45.395802
3504.012453	361609.825059	45.400807
3504.022046	361616.388459	45.405812
3503.896379	361626.866368	45.410817
3503.726259	361607.020521	45.415821
3503.900315	361614.575735	45.420826
3503.962987	361623.268148	45.425831
3503.847590	361625.118482	45.430836
3503.962996	361613.777118	45.435841
3503.951939	361623.269989	45.440845
3503.964455	361614.692981	45.445850
3504.157220	361631.710882	45.450855
3504.129108	361627.974901	45.455860
3504.140789	361625.072323	45.460865
3503.807569	361617.924013	45.465869
3504.248547	361613.019732	45.470874
3504.103669	361600.930705	45.475879
3503.976055	361597.973810	45.480884
3504.131309	361616.371692	45.485889
3504.146559	361617.514351	45.490893
3504.316218	361617.869243	45.495898
3504.219819	361598.495200	45.500903
3504.040324	361577.098659	45.505908
3504.487146	361579.725262	45.510913
3503.803700	361568.204822	45.515917
3504.415294	361567.573824	45.520922
3504.232286	361594.981935	45.525927
3504.198402	361564.071274	45.530932
3504.542888	361533.329789	45.535937
3504.019121	361535.092007	45.540941
3504.095717	361533.400539	45.545946
3504.446843	361545.533379	45.550951
3504.272288	361540.599164	45.555956
3503.982904	361507.362438	45.560961
3503.900488	361508.393312	45.565965
3504.061879	361511.192265	45.570970
3504.224843	361509.716151	45.575975
3503.669202	361508.099177	45.580980
3504.068175	361510.122660	45.585985
3504.060622	361509.894877	45.590989
3503.878604	361501.145036	45.595994
3504.023153	361520.638798	45.600999
3503.718835	361513.180558	45.606004
3504.033475	361498.041762	45.611009
3504.173054	361508.681331	45.616013
3504.022478	361503.336196	45.621018
3503.931657	361488.744952	45.626023
3503.727478	361487.733999	45.631028
3504.054428	361470.328611	45.636033
3504.065932	361477.146182	45.641037
3504.112883	361477.520472	45.646042
3504.006147	361483.262583	45.651047
3503.845127	361482.397480	45.656052
3504.032632	361480.917486	45.661057
3503.998470	361486.978913	45.666061
3504.057999	361473.966955	45.671066
3503.801252	361466.272180	45.676071
3503.721314	361454.096515	45.681076
3504.152685	361455.555080	45.686081
3504.094897	361453.299608	45.691085
3504.282645	361447.671978	45.696090
3504.151305	361455.402720	45.701095
3504.319085	361447.259155	45.706100
3504.542079	361446.206122	45.711105
3504.280877	361429.504380	45.716109
3504.074492	361416.712558	45.721114
3504.010986	361435.094200	45.726119
3504.119658	361423.244948	45.731124
3504.084776	361408.339491	45.736129
3503.889452	361420.380626	45.741133
3504.014923	361433.490645	45.746138
3504.291682	361420.291661	45.751143
3504.192676	361394.785607	45.756148
3504.322734	361395.273987	45.761153
3503.911545	361388.417866	45.766157
3504.088790	361375.387273	45.771162
3504.146116	361379.576737	45.776167
3504.039372	361386.591131	45.781172
3504.438203	361379.377956	45.786177
3504.199064	361362.647258	45.791181
3503.979669	361344.361261	45.796186
3504.058302	361371.092006	45.801191
3504.120231	361360.115271	45.806196
3503.898066	361351.066404	45.811201
3503.625357	361363.145231	45.816205
3503.700686	361364.634635	45.821210
3503.644836	361372.048113	45.826215
3503.835146	361366.318287	45.831220
3503.794188	361368.182308	45.836225
3504.073152	361374.957615	45.841229
3504.132974	361357.721639	45.846234
3504.042873	361369.135463	45.851239
3503.995736	361363.977526	45.856244
3504.128697	361333.600139	45.861249
3504.068993	361339.920077	45.866253
3504.125260	361343.193675	45.871258
3504.159374	361339.702290	45.876263
3503.820920	361336.702370	45.881268
3504.208489	361337.099154	45.886273
3503.794537	361352.075646	45.891277
3503.878422	361339.339700	45.896282
3503.643237	361339.936709	45.901287
3503.768477	361363.479411	45.906292
3504.092989	361334.013226	45.911297
3503.632815	361349.073362	45.916301
3504.041345	361349.848514	45.921306
3504.045090	361328.092105	45.926311
3503.954940	361309.963783	45.931316
3504.034488	361312.623012	45.936321
3503.989809	361318.864241	45.941325
3504.047854	361314.402144	45.946330
3503.891028	361305.292048	45.951335
3503.693873	361320.107052	45.956340
3503.842318	361312.271865	45.961345
3503.590051	361328.037060	45.966349
3503.609452	361317.219711	45.971354
3503.957110	361319.480322	45.976359
3503.552473	361324.124497	45.981364
3503.896897	361327.505218	45.986369
3503.804396	361334.364696	45.991373
3504.244450	361333.379130	45.996378
3503.974703	361334.668628	46.001383
3503.990796	361312.477688	46.006388
3503.865874	361326.238008	46.011393
3503.979880	361320.800138	46.016397
3503.918543	361330.224680	46.021402
3504.203063	361329.212809	46.026407
3504.033427	361290.359004	46.031412
3504.106694	361305.054930	46.036417
3503.995971	361282.807685	46.041421
3504.101140	361285.717321	46.046426
3504.001602	361305.758664	46.051431
3503.798670	361288.996771	46.056436
3504.015462	361292.295889	46.061441
3503.871464	361304.710621	46.066445
3504.289511	361303.041506	46.071450
3504.173663	361283.517736	46.076455
3503.928885	361263.988893	46.081460
3504.323716	361265.987595	46.086465
3504.009054	361279.243567	46.091469
3504.193399	361256.084521	46.096474
3504.326676	361287.615871	46.101479
3504.268984	361240.474554	46.106484
3504.245997	361244.727616	46.111489
3504.120389	361237.470093	46.116493
3504.082666	361230.020558	46.121498
3503.644061	361228.156064	46.126503
3503.788367	361230.372488	46.131508
3503.805453	361219.911719	46.136513
3503.803359	361241.031843	46.141517
3504.074693	361217.146553	46.146522
3503.790826	361231.008363	46.151527
3503.644223	361242.329367	46.156532
3504.120058	361231.872421	46.161537
3503.765619	361241.750440	46.166541
3503.734771	361236.488131	46.171546
3503.830317	361237.592661	46.176551
3503.932632	361247.347587	46.181556
3504.367965	361237.762190	46.186561
3504.047679	361226.769506	46.191565
3503.776141	361213.758920	46.196570
3503.861453	361217.765855	46.201575
3503.922731	361207.145425	46.206580
3504.120505	361205.231225	46.211585
3504.001861	361210.110104	46.216589
3503.875055	361229.875889	46.221594
3503.831111	361216.727544	46.226599
3503.793431	361218.667390	46.231604
3503.696258	361227.563261	46.236609
3503.929365	361229.460302	46.241613
3503.719995	361223.081164	46.246618
3503.674643	361227.821227	46.251623
3503.459652	361218.618528	46.256628
3503.862550	361226.035848	46.261633
3503.791717	361224.011436	46.266637
3503.747107	361224.476539	46.271642
3503.957652	361229.048923	46.276647
3503.716605	361249.239887	46.281652
3504.219142	361228.575078	46.286657
3504.054480	361230.076977	46.291661
3503.727375	361226.897138	46.296666
3504.003783	361248.889271	46.301671
3503.944300	361230.298052	46.306676
3503.949196	361226.963950	46.311681
3503.860897	361226.825266	46.316685
3503.743243	361206.258485	46.321690
3504.022960	361204.331332	46.326695
3503.922397	361212.693387	46.331700
3504.280302	361201.949729	46.336705
3504.111598	361211.467603	46.341709
3504.234216	361204.323510	46.346714
3504.371427	361207.838777	46.351719
3504.145511	361202.581855	46.356724
3503.956120	361186.097685	46.361729
3503.826619	361179.069779	46.366733
3504.009591	361178.786432	46.371738
3504.062006	361175.292141	46.376743
3504.047557	361179.213067	46.381748
3504.313923	361189.323755	46.386753
3503.935900	361189.561662	46.391757
3504.388616	361183.255978	46.396762
3504.377448	361167.710559	46.401767
3504.322462	361161.841365	46.406772
3504.258921	361156.329761	46.411777
3504.034070	361132.446527	46.416781
3504.232182	361156.486724	46.421786
3504.329559	361133.392257	46.426791
3504.030612	361126.620138	46.431796
3504.025810	361112.142408	46.436801
3503.841089	361101.815296	46.441805
3504.005066	361122.120408	46.446810
3504.201655	361099.315588	46.451815
3503.687635	361126.012927	46.456820
3504.088690	361105.974800	46.461825
3503.565026	361118.296924	46.466829
3503.997899	361126.930908	46.471834
3503.987482	361108.357331	46.476839
3503.863779	361134.763955	46.481844
3504.125723	361120.065943	46.486849
3503.621988	361124.878475	46.491853
3504.198810	361101.937215	46.496858
3504.187471	361087.282392	46.501863
3504.101068	361089.942421	46.506868
3504.304407	361081.487825	46.511873
3504.093808	361080.121641	46.516877
3504.396347	361073.865128	46.521882
3504.066799	361075.647552	46.526887
3503.822516	361083.727000	46.531892
3504.517768	361055.906892	46.536897
3503.929940	361047.602800	46.541901
3504.015409	361074.688870	46.546906
3504.089070	361055.389505	46.551911
3503.701147	361061.176115	46.556916
3503.962053	361058.132324	46.561921
3503.989324	361060.596267	46.566925
3503.839454	361054.182255	46.571930
3503.906599	361068.701102	46.576935
3504.033053	361041.250800	46.581940
3504.241175	361047.604777	46.586945
3503.773844	361038.849060	46.591949
3503.682233	361022.934627	46.596954
3504.269134	361027.574766	46.601959
3503.997173	361039.780785	46.606964
3504.028267	361018.808725	46.611969
3503.911380	361027.326065	46.616973
3504.096359	361022.742093	46.621978
3503.948581	361035.844525	46.626983
3503.627559	361039.203230	46.631988
3503.917321	361024.577127	46.636993
3504.015231	361041.635680	46.641997
3504.203855	361023.335953	46.647002
3504.015649	360995.604572	46.652007
3503.783104	361010.476157	46.657012
3503.956728	360990.957400	46.662017
3503.912932	360988.928705	46.667021
3504.035046	361001.454124	46.672026
3504.367266	360979.213056	46.677031
3503.965186	360990.065592	46.682036
3504.282425	360993.043505	46.687041
3504.155607	361004.005200	46.692045
3503.956258	360975.512199	46.697050
3504.304015	360961.869290	46.702055
3504.002224	360954.995814	46.707060
3503.893474	360960.636522	46.712065
3503.504287	360974.642283	46.717069
3503.893596	360970.509473	46.722074
3503.628046	360957.879554	46.727079
3503.640372	360971.643727	46.732084
3504.080630	360945.772285	46.737089
3503.934450	360964.014504	46.742093
3503.922329	360970.708654	46.747098
3503.964132	360969.429796	46.752103
3504.272245	360971.111425	46.757108
3504.209394	360956.362922	46.762113
3503.917691	360970.124264	46.767117
3503.887519	360965.726970	46.772122
3503.967436	360946.401127	46.777127
3503.583012	360948.777480	46.782132
3503.905407	360922.517527	46.787137
3503.893003	360945.395161	46.792141
3503.959717	360924.646440	46.797146
3503.963884	360947.623237	46.802151
3503.521969	360956.446426	46.807156
3503.956803	360943.833018	46.812161
3503.693001	360933.594707	46.817165
3503.594325	360962.414808	46.822170
3503.978401	360951.717849	46.827175
3503.915772	360946.714988	46.832180
3504.116520	360953.528165	46.837185
3503.774223	360950.681502	46.842189
3503.957263	360963.528094	46.847194
3503.935709	360956.788438	46.852199
3503.891279	360946.897137	46.857204
3504.127795	360962.534297	46.862209
3504.105752	360943.300907	46.867213
3503.824872	360969.019991	46.872218
3503.948817	360949.152831	46.877223
3503.463027	360974.039151	46.882228
3504.101466	360942.182102	46.887233
3503.647430	360984.493664	46.892237
3504.183661	360941.762042	46.897242
3503.848487	360962.782266	46.902247
3503.721296	360913.183384	46.907252
3504.022099	360896.952421	46.912257
3503.607138	360940.555574	46.917261
3503.983159	360908.663647	46.922266
3503.985802	360925.126605	46.927271
3503.888611	360918.297117	46.932276
3503.987092	360934.490465	46.937281
3503.999907	360909.704399	46.942285
3503.887444	360945.549692	46.947290
3503.769351	360920.606205	46.952295
3503.849367	360930.746405	46.957300
3504.174007	360937.005642	46.962305
3503.854369	360945.198808	46.967309
3504.092906	360921.852914	46.972314
3504.198493	360940.513365	46.977319
3503.948502	360911.239517	46.982324
3504.063663	360915.394433	46.987329
3504.050360	360887.329993	46.992333
3504.295571	360898.614588	46.997338
3504.036297	360887.815747	47.002343
3503.898238	360924.632038	47.007348
3504.146904	360888.459913	47.012353
3503.964750	360915.206693	47.017357
3504.309849	360887.314609	47.022362
3504.386818	360881.907990	47.027367
3503.859833	360871.533149	47.032372
3504.068336	360853.993586	47.037377
3504.097190	360864.141888	47.042381
3504.244238	360872.286740	47.047386
3504.012925	360857.564837	47.052391
3503.571120	360888.907454	47.057396
3503.893305	360845.318983	47.062401
3503.732706	360894.861708	47.067405
3503.926899	360861.191850	47.072410
3504.120779	360872.739022	47.077415
3504.137208	360847.519775	47.082420
3504.008714	360817.539630	47.087425
3504.086651	360849.105464	47.092429
3504.018951	360832.881839	47.097434
3503.973062	360840.955412	47.102439
3503.813512	360825.891361	47.107444
3504.186465	360821.964690	47.112449
3503.925883	360845.288734	47.117453
3504.098816	360840.681203	47.122458
3504.092170	360828.366563	47.127463
3503.662373	360817.569216	47.132468
3504.173825	360799.778179	47.137473
3503.973667	360797.087158	47.142477
3504.137639	360804.796770	47.147482
3504.134838	360794.847965	47.152487
3503.812590	360818.970588	47.157492
3504.106018	360789.967004	47.162497
3503.759695	360795.110927	47.167501
3503.948944	360804.852201	47.172506
3504.107568	360803.020512	47.177511
3503.991009	360801.588562	47.182516
3504.274664	360803.146835	47.187521
3503.973551	360799.657510	47.192525
3504.173357	360773.238733	47.197530
3503.879223	360771.147818	47.202535
3503.615455	360782.283886	47.207540
3503.957128	360781.008512	47.212545
3504.154545	360780.264857	47.217549
3504.091448	360781.012789	47.222554
3504.369620	360781.426871	47.227559
3504.200628	360764.913886	47.232564
3504.149230	360738.483908	47.237569
3503.996587	360733.749712	47.242573
3503.708744	360734.100593	47.247578
3504.025433	360739.801305	47.252583
3503.988765	360752.809913	47.257588
3504.071135	360732.287645	47.262593
3503.965618	360750.676192	47.267597
3503.917315	360751.065545	47.272602
3504.013761	360754.587290	47.277607
3504.119403	360742.916468	47.282612
3504.097385	360733.097918	47.287617
3503.731359	360722.723046	47.292621
3503.904323	360713.026345	47.297626
3504.033839	360723.158765	47.302631
3504.035578	360727.128060	47.307636
3503.964834	360705.434034	47.312641
3503.688609	360729.142295	47.317645
3503.851534	360704.408730	47.322650
3504.075957	360711.269091	47.327655
3503.737835	360724.783382	47.332660
3504.122523	360720.091475	47.337665
3504.050258	360720.866303	47.342669
3503.994007	360715.022699	47.347674
3504.203948	360731.223943	47.352679
3503.721695	360703.487982	47.357684
3504.267624	360682.612512	47.362689
3503.978072	360687.442122	47.367693
3503.544485	360686.798211	47.372698
3503.745043	360692.008371	47.377703
3504.002347	360687.489271	47.382708
3504.327083	360672.806642	47.387713
3504.057778	360686.030162	47.392717
3504.004945	360705.886254	47.397722
3504.354292	360677.230003	47.402727
3503.894024	360696.845154	47.407732
3503.972443	360682.939392	47.412737
3504.042899	360686.770600	47.417741
3503.939608	360684.140598	47.422746
3504.244335	360665.746044	47.427751
3503.923681	360655.313094	47.432756
3503.880343	360662.673812	47.437761
3503.895029	360660.890317	47.442765
3503.638089	360652.228500	47.447770
3503.660589	360667.594238	47.452775
3503.599154	360663.303641	47.457780
3503.752315	360662.185292	47.462785
3503.980779	360655.991326	47.467789
3503.663854	360669.527728	47.472794
3503.920272	360655.008567	47.477799
3503.536226	360685.171681	47.482804
3504.234733	360649.895207	47.487809
3503.833501	360679.628462	47.492813
3504.424864	360664.903683	47.497818
3503.987360	360673.344540	47.502823
3504.110166	360643.858922	47.507828
3504.117217	360649.863050	47.512833
3503.755162	360661.828948	47.517837
3503.979534	360625.914923	47.522842
3503.809484	360651.336754	47.527847
3503.466243	360637.319513	47.532852
3504.251435	360620.681090	47.537857
3503.834314	360653.063239	47.542861
3503.850620	360615.426336	47.547866
3504.209561	360652.266056	47.552871
3504.162496	360629.982999	47.557876
3504.394982	360635.340793	47.562881
3504.276849	360657.090217	47.567885
3504.254229	360604.700892	47.572890
3503.936458	360604.394914	47.577895
3503.958386	360618.106779	47.582900
3504.511314	360584.736260	47.587905
3504.220433	360626.869672	47.592909
3504.407455	360604.066129	47.597914
3504.142503	360577.924278	47.602919
3503.948020	360580.499637	47.607924
3503.835309	360554.333708	47.612929
3503.898887	360580.558358	47.617933
3503.830318	360565.021818	47.622938
3503.447137	360573.708563	47.627943
3503.841128	360563.111733	47.632948
3503.767039	360573.581720	47.637953
3503.995404	360551.153304	47.642957
3503.965859	360588.029038	47.647962
3503.920166	360548.544337	47.652967
3504.090095	360577.474884	47.657972
3504.168398	360555.553663	47.662977
3503.908932	360586.638642	47.667981
3504.089296	360558.797853	47.672986
3503.932423	360565.514941	47.677991
3503.867442	360540.130281	47.682996
3504.010068	360534.178880	47.688001
3503.752488	360532.158514	47.693005
3503.583796	360526.536229	47.698010
3503.982840	360546.091943	47.703015
3503.747558	360522.260945	47.708020
3503.993840	360535.072209	47.713025
3504.027407	360552.573686	47.718029
3503.891026	360530.762727	47.723034
3504.089935	360541.622146	47.728039
3503.926877	360539.434163	47.733044
3503.773708	360552.512132	47.738049
3504.408640	360533.530968	47.743053
3504.034651	360551.605788	47.748058
3504.051144	360531.959007	47.753063
3503.838137	360503.366101	47.758068
3503.887174	360510.661349	47.763073
3504.043584	360511.552707	47.768077
3503.862279	360497.942406	47.773082
3503.813794	360516.881837	47.778087
3503.802396	360511.769049	47.783092
3503.883218	360499.262377	47.788097
3503.796058	360516.935627	47.793101
3503.770548	360506.735894	47.798106
3503.856928	360512.905619	47.803111
3503.881410	360517.074905	47.808116
3503.781412	360509.456980	47.813121
3503.904184	360531.066597	47.818125
3504.089419	360525.464702	47.823130
3504.158041	360505.606103	47.828135
3503.653949	360538.689115	47.833140
3504.101511	360509.940902	47.838145
3504.098094	360511.010201	47.843149
3503.779776	360529.178012	47.848154
3504.051802	360503.612830	47.853159
3503.664979	360482.528477	47.858164
3503.650678	360500.088432	47.863169
3503.853958	360474.076075	47.868173
3503.737013	360502.848449	47.873178
3504.018879	360486.951137	47.878183
3503.630810	360492.330703	47.883188
3503.924500	360490.655773	47.888193
3503.884712	360475.623571	47.893197
3503.989842	360498.126598	47.898202
3503.814837	360509.630386	47.903207
3503.895248	360477.581335	47.908212
3504.148028	360515.837466	47.913217
3503.341074	360503.038550	47.918221
3503.869745	360482.471072	47.923226
3503.710847	360509.901441	47.928231
3503.818716	360479.731045	47.933236
3503.854323	360514.306406	47.938241
3503.589299	360502.770457	47.943245
3503.267418	360516.256794	47.948250
3503.732988	360491.729738	47.953255
3503.738425	360516.564091	47.958260
3503.963394	360502.431543	47.963265
3503.740806	360502.848449	47.968269
3503.754646	360519.360667	47.973274
3504.177916	360504.102601	47.978279
3503.782774	360504.445000	47.983284
3504.217043	360507.811578	47.988289
3503.999402	360515.225318	47.993293
3504.073028	360533.789196	47.998298
3503.947152	360505.513315	48.003303
3503.979304	360493.650482	48.008308
3503.988282	360526.983195	48.013313
3504.142622	360502.021870	48.018317
3503.976356	360512.888129	48.023322
3504.104191	360472.001858	48.028327
3503.714773	360496.440611	48.033332
3504.196308	360465.371425	48.038337
3503.963841	360483.907371	48.043341
3504.109949	360474.571109	48.048346
3504.268974	360458.896774	48.053351
3504.031119	360484.965559	48.058356
3504.199811	360455.905153	48.063361
3504.080882	360453.023151	48.068365
3504.389482	360443.254062	48.073370
3504.128122	360425.534157	48.078375
3503.853929	360454.356862	48.083380
3504.100788	360427.854120	48.088385
3503.928115	360452.207742	48.093389
3504.333752	360436.570754	48.098394
3504.098353	360447.575185	48.103399
3504.128610	360405.813675	48.108404
3503.981247	360427.109797	48.113409
3503.823138	360399.780447	48.118413
3503.866200	360407.305668	48.123418
3504.060347	360424.120215	48.128423
3503.965519	360401.106669	48.133428
3503.717184	360424.149077	48.138433
3504.136003	360394.209380	48.143437
3503.863519	360421.072497	48.148442
3503.946075	360402.789301	48.153447
3504.077241	360412.310823	48.158452
3503.880304	360402.850653	48.163457
3503.739784	360380.378685	48.168461
3503.401337	360376.742554	48.173466
3503.789003	360406.605732	48.178471
3503.714240	360399.823517	48.183476
3503.721586	360409.161046	48.188481
3503.964303	360438.716319	48.193485
3503.923761	360408.442110	48.198490
3503.791268	360422.331116	48.203495
3503.404039	360413.206379	48.208500
3503.520111	360428.582848	48.213505
3503.957976	360401.922668	48.218509
3503.584453	360425.595567	48.223514
3503.925875	360429.740205	48.228519
3503.799387	360414.365447	48.233524
3503.464970	360434.240716	48.238529
3503.760441	360419.155501	48.243533
3503.948188	360416.046897	48.248538
3504.061577	360445.571718	48.253543
3503.733456	360429.440014	48.258548
3503.592737	360441.930790	48.263553
3503.890346	360428.015751	48.268557
3503.852420	360445.452232	48.273562
3504.032203	360425.423352	48.278567
3504.165361	360446.420663	48.283572
3504.236874	360405.797697	48.288577
3503.967866	360414.161072	48.293581
3504.003948	360407.055985	48.298586
3504.122578	360407.215385	48.303591
3503.696771	360423.771688	48.308596
3504.077906	360385.389895	48.313601
3503.970207	360420.318774	48.318605
3503.808093	360402.837631	48.323610
3504.152258	360412.910740	48.328615
3503.652133	360396.500864	48.333620
3503.792849	360424.952648	48.338625
3503.710893	360418.985843	48.343629
3503.861003	360405.475803	48.348634
3503.790710	360418.388033	48.353639
3503.623832	360412.536434	48.358644
3503.970921	360401.794307	48.363649
3503.877731	360431.122779	48.368653
3503.889818	360389.796708	48.373658
3503.761445	360356.482836	48.378663
3503.809498	360404.339098	48.383668
3503.749626	360368.062678	48.388673
3503.691332	360380.438656	48.393677
3503.823859	360366.473357	48.398682
3503.766894	360381.877194	48.403687
3503.439897	360380.427605	48.408692
3503.911608	360401.422310	48.413697
3503.740473	360403.281501	48.418701
3503.496301	360433.880688	48.423706
3503.682434	360438.889588	48.428711
3504.187398	360410.132242	48.433716
3503.960500	360445.436188	48.438721
3503.988869	360386.371736	48.443725
3504.026701	360405.602917	48.448730
3504.233976	360365.976294	48.453735
3504.027912	360387.358050	48.458740
3503.796351	360369.862428	48.463745
3503.949130	360400.831469	48.468749
3503.807266	360377.876240	48.473754
3504.305752	360382.250514	48.478759
3503.944306	360403.376920	48.483764
3503.958174	360383.297913	48.488769
3503.859943	360393.797200	48.493773
3503.756543	360379.360281	48.498778
3504.311315	360346.345549	48.503783
3503.566638	360381.604161	48.508788
3504.020821	360339.673797	48.513793
3503.973215	360372.404858	48.518797
3503.983326	360370.622075	48.523802
3503.921807	360345.033196	48.528807
3504.132198	360376.934647	48.533812
3504.312427	360346.778176	48.538817
3504.237585	360374.144442	48.543821
3504.702869	360321.066980	48.548826
3504.659098	360339.166018	48.553831
3504.015098	360323.338671	48.558836
3503.974132	360326.475033	48.563841
3503.932582	360348.772302	48.568845
3503.744215	360325.697170	48.573850
3504.095619	360305.895571	48.578855
3504.049536	360299.770404	48.583860
3503.745193	360318.190546	48.588865
3503.523660	360298.733972	48.593869
3503.812439	360286.855968	48.598874
3503.508940	360314.080292	48.603879
3503.744093	360299.640723	48.608884
3504.019725	360317.765617	48.613889
3504.046917	360322.239843	48.618893
3503.981652	360289.094071	48.623898
3504.075387	360311.217296	48.628903
3503.575953	360298.802296	48.633908
3504.118805	360298.970976	48.638913
3504.019145	360295.882350	48.643917
3503.801397	360296.527506	48.648922
3504.317561	360294.283036	48.653927
3503.707084	360303.285665	48.658932
3504.130531	360302.251813	48.663937
3504.012655	360314.789902	48.668941
3504.349133	360298.069624	48.673946
3504.109077	360282.102072	48.678951
3503.739673	360279.997587	48.683956
3503.807493	360271.437041	48.688961
3504.037819	360235.954366	48.693965
3503.885801	360280.687071	48.698970
3504.044501	360293.232338	48.703975
3503.954258	360303.603153	48.708980
3503.872099	360273.997033	48.713985
3503.637058	360273.118162	48.718989
3504.106135	360254.621134	48.723994
3504.292085	360262.429143	48.728999
3503.758228	360282.005204	48.734004
3503.763203	360265.948021	48.739009
3504.137254	360237.669293	48.744013
3503.846332	360248.987899	48.749018
3503.961585	360264.975254	48.754023
3503.628525	360251.287088	48.759028
3504.162645	360207.969888	48.764033
3504.075833	360247.170525	48.769037
3503.568260	360251.500277	48.774042
3504.248428	360221.951742	48.779047
3503.670212	360255.173896	48.784052
3503.921302	360219.738819	48.789057
3504.008013	360244.942154	48.794061
3503.585517	360248.291509	48.799066
3504.333273	360223.465249	48.804071
3503.556976	360249.288478	48.809076
3504.041972	360236.921416	48.814081
3503.737289	360235.061159	48.819085
3504.030581	360246.592768	48.824090
3504.361672	360229.211720	48.829095
3503.816764	360214.488299	48.834100
3503.794992	360221.311309	48.839105
3503.945431	360211.083700	48.844109
3503.689370	360192.268692	48.849114
3504.108406	360213.042791	48.854119
3504.022327	360203.870410	48.859124
3503.809966	360205.176313	48.864129
3504.202176	360184.045020	48.869133
3504.082846	360229.663216	48.874138
3503.896413	360230.125301	48.879143
3503.417982	360211.727142	48.884148
3504.097536	360205.792610	48.889153
3504.125851	360233.142650	48.894157
3503.522418	360214.458900	48.899162
3504.155958	360207.666477	48.904167
3503.598312	360226.737399	48.909172
3503.885251	360205.673649	48.914177
3503.838135	360213.085925	48.919181
3503.575894	360235.774377	48.924186
3504.083982	360204.802609	48.929191
3504.170866	360231.634471	48.934196
3503.991011	360196.292945	48.939201
3504.455456	360157.719679	48.944205
3504.138193	360198.865239	48.949210
3504.116917	360216.909875	48.954215
3504.224788	360199.971239	48.959220
3504.091937	360191.086155	48.964225
3503.837082	360162.881353	48.969229
3504.052754	360118.723800	48.974234
3504.153096	360156.673514	48.979239
3503.584337	360154.142508	48.984244
3504.134218	360123.494881	48.989249
3503.944962	360168.564375	48.994253
3503.885460	360163.866291	48.999258
3503.807741	360150.850223	49.004263
3503.880661	360151.576664	49.009268
3504.251585	360117.954686	49.014273
3503.935575	360171.695882	49.019277
3503.450330	360157.319256	49.024282
3503.929490	360136.148752	49.029287
3503.664651	360145.758371	49.034292
3504.286131	360135.812532	49.039297
3504.065624	360138.748273	49.044301
3504.195685	360106.462111	49.049306
3504.329779	360134.864222	49.054311
3503.928118	360140.042407	49.059316
3503.315786	360118.459174	49.064321
3503.559494	360106.181112	49.069325
3503.810061	360098.634938	49.074330
3504.295956	360086.165911	49.079335
3504.120660	360106.932221	49.084340
3503.980535	360146.879304	49.089345
3504.071406	360129.230841	49.094349
3503.768444	360112.789701	49.099354
3504.235717	360087.575126	49.104359
3504.133938	360080.135538	49.109364
3503.986256	360083.008879	49.114369
3503.706293	360073.943459	49.119373
3503.981326	360110.618736	49.124378
3503.947564	360087.086466	49.129383
3503.535958	360089.060020	49.134388
3503.533225	360089.722082	49.139393
3503.893827	360072.997913	49.144397
3503.463548	360083.727879	49.149402
3504.025473	360090.916670	49.154407
3503.732457	360096.586608	49.159412
3504.152350	360097.156417	49.164417
3503.719933	360098.522554	49.169421
3503.767573	360100.372620	49.174426
3503.988435	360104.434559	49.179431
3504.036094	360122.010304	49.184436
3503.740331	360119.868725	49.189441
3504.015185	360115.855720	49.194445
3503.980719	360087.717819	49.199450
3504.195118	360085.190242	49.204455
3504.118492	360118.409539	49.209460
3503.845295	360104.762760	49.214465
3503.626711	360092.812233	49.219469
3504.125311	360070.544445	49.224474
3504.181315	360046.489043	49.229479
3503.546782	360036.487267	49.234484
3503.750698	360036.607741	49.239489
3503.658590	360057.997076	49.244493
3503.213176	360073.386077	49.249498
3503.621774	360084.136114	49.254503
3503.570604	360101.473028	49.259508
3503.426999	360096.279310	49.264513
3504.313503	360073.593960	49.269517
3503.812541	360117.058778	49.274522
3504.034493	360111.909061	49.279527
3503.485194	360105.100032	49.284532
3504.228846	360084.600186	49.289537
3504.331487	360071.173894	49.294541
3503.956360	360055.685649	49.299546
3504.014664	360060.282211	49.304551
3503.846903	360092.319965	49.309556
3504.071397	360068.823200	49.314561
3503.828394	360069.294228	49.319565
3503.671799	360108.989485	49.324570
3504.103095	360097.954073	49.329575
3504.025605	360080.179529	49.334580
3504.547887	360049.129080	49.339585
3504.232386	360029.000206	49.344589
3504.021030	360064.072960	49.349594
3503.950463	360043.371005	49.354599
3503.867043	360032.060696	49.359604
3503.896705	360013.887498	49.364609
3503.742405	360056.406957	49.369613
3504.027004	360066.616785	49.374618
3504.168916	360052.293666	49.379623
3503.346829	360049.191992	49.384628
3503.930259	360020.014871	49.389633
3504.134172	359999.345847	49.394637
3503.867350	360052.290570	49.399642
3504.017173	360036.693890	49.404647
3503.812700	360061.968797	49.409652
3503.907882	360025.184132	49.414657
3503.948902	360053.448326	49.419661
3503.710858	360032.543826	49.424666
3504.384656	360034.702052	49.429671
3504.152297	360008.961878	49.434676
3503.459464	360009.783921	49.439681
3504.231092	359985.335459	49.444685
3504.034804	359989.387011	49.449690
3504.192631	360016.487686	49.454695
3503.684720	360005.575272	49.459700
3503.600838	360004.418041	49.464705
3503.923298	359996.962271	49.469709
3503.359116	360029.088177	49.474714
3503.669617	360007.613478	49.479719
3503.812563	360006.216821	49.484724
3504.053342	360023.583951	49.489729
3504.139464	360023.214123	49.494733
3503.682895	360010.130673	49.499738
3504.141238	360005.376161	49.504743
3503.807345	360032.020187	49.509748
3504.115716	359999.909337	49.514753
3504.044542	359996.510836	49.519757
3503.667678	359995.628933	49.524762
3503.990341	359982.193282	49.529767
3503.815324	359974.179993	49.534772
3503.973112	359986.216562	49.539777
3503.782661	359961.258568	49.544781
3503.632947	359977.924057	49.549786
3503.593218	359996.200708	49.554791
3503.614610	359972.914125	49.559796
3503.906620	359984.496892	49.564801
3503.845945	360010.563371	49.569805
3503.579608	359980.222801	49.574810
3504.085066	359962.686864	49.579815
3503.964660	360015.608482	49.584820
3503.958761	359966.243910	49.589825
3503.949219	359994.236224	49.594829
3503.774626	359993.144224	49.599834
3504.485281	359954.582768	49.604839
3504.276264	360009.426863	49.609844
3504.160277	359996.416802	49.614849
3504.380338	359979.638478	49.619853
3503.999676	359960.563168	49.624858
3503.958605	359953.775564	49.629863
3503.685470	359967.763272	49.634868
3503.898823	359937.830325	49.639873
3504.049497	359980.810565	49.644877
3503.603925	359970.600781	49.649882
3504.043768	359941.573542	49.654887
3503.779073	359976.171313	49.659892
3503.894864	359937.780216	49.664897
3504.197075	359959.743417	49.669901
3503.852948	359946.438606	49.674906
3504.084177	359920.930457	49.679911
3504.127192	359968.228132	49.684916
3504.077360	359957.701327	49.689921
3503.827398	359934.686636	49.694925
3503.543728	359919.896382	49.699930
3503.906933	359899.227582	49.704935
3504.061771	359901.238833	49.709940
3503.636930	359933.978931	49.714945
3503.944322	359893.267355	49.719949
3503.780532	359928.739827	49.724954
3503.881149	359895.694793	49.729959
3503.944242	359940.928179	49.734964
3504.126265	359932.629428	49.739969
3503.998269	359916.389579	49.744973
3504.078413	359897.979341	49.749978
3504.313266	359899.748929	49.754983
3503.884751	359953.177351	49.759988
3503.488629	359913.416724	49.764993
3504.028713	359887.528934	49.769997
3504.024129	359923.765075	49.775002
3504.132397	359882.906843	49.780007
3503.850294	359902.290584	49.785012
3503.887935	359874.548300	49.790017
3503.929169	359889.885878	49.795021
3503.696875	359899.337725	49.800026
3503.566344	359889.459817	49.805031
3503.945888	359876.803978	49.810036
3503.571468	359916.330256	49.815041
3503.866457	359884.959385	49.820045
3503.939199	359901.080811	49.825050
3503.524973	359896.311544	49.830055
3504.076709	359874.824098	49.835060
3504.021861	359908.447237	49.840065
3503.935377	359905.560073	49.845069
3503.705242	359902.288477	49.850074
3504.360245	359890.072576	49.855079
3504.268769	359895.379879	49.860084
3504.056769	359894.879052	49.865089
3504.227247	359856.810046	49.870093
3503.929764	359871.768587	49.875098
3504.374197	359859.102486	49.880103
3503.675342	359867.788366	49.885108
3504.172540	359829.998494	49.890113
3504.333113	359881.298176	49.895117
3503.808385	359864.357637	49.900122
3504.430638	359812.908807	49.905127
3504.319014	359847.482474	49.910132
3503.677253	359833.308616	49.915137
3504.171529	359810.659699	49.920141
3504.146146	359822.954279	49.925146
3504.207745	359849.026963	49.930151
3503.954599	359848.481747	49.935156
3504.425354	359811.688444	49.940161
3504.214703	359821.747594	49.945165
3503.926691	359785.175998	49.950170
3504.022141	359809.742023	49.955175
3504.048091	359775.767200	49.960180
3503.802071	359806.646985	49.965185
3504.100441	359793.469585	49.970189
3503.685764	359786.232091	49.975194
3504.052922	359804.317264	49.980199
3503.962400	359789.903578	49.985204
3503.758937	359807.977166	49.990209
3504.138172	359788.858006	49.995213
3503.839865	359802.544385	50.000218
3504.376554	359774.239678	50.005223
3504.197227	359768.975233	50.010228
3504.107183	359760.770353	50.015233
3504.159666	359748.980462	50.020237
3503.722707	359779.915894	50.025242
3504.341467	359725.566650	50.030247
3504.033359	359774.268672	50.035252
3504.373858	359739.480713	50.040257
3503.820211	359744.301271	50.045261
3503.692308	359707.755199	50.050266
3503.813546	359719.085115	50.055271
3503.802447	359705.956611	50.060276
3503.685193	359728.266134	50.065281
3503.686275	359717.476766	50.070285
3503.877057	359707.878831	50.075290
3503.983095	359723.333449	50.080295
3503.850207	359712.616150	50.085300
3503.854746	359745.110377	50.090305
3504.215943	359712.990986	50.095309
3503.835671	359722.313581	50.100314
3504.146117	359731.170741	50.105319
3503.904151	359719.987207	50.110324
3503.885764	359733.654803	50.115329
3503.985354	359718.549441	50.120333
3503.726632	359737.166163	50.125338
3503.667011	359706.182033	50.130343
3503.753455	359736.831184	50.135348
3503.968979	359713.691913	50.140353
3503.581736	359741.769525	50.145357
3503.649698	359710.307196	50.150362
3503.869371	359745.159368	50.155367
3503.989016	359734.325815	50.160372
3503.572402	359736.325621	50.165377
3503.635262	359741.583097	50.170381
3503.651376	359718.729813	50.175386
3504.142364	359743.284240	50.180391
3503.976707	359720.459690	50.185396
3503.801320	359731.912831	50.190401
3503.870584	359718.644396	50.195405
3503.660108	359713.944687	50.200410
3503.770493	359725.963367	50.205415
3504.081579	359749.604716	50.210420
3503.742135	359721.642043	50.215425
3503.773575	359714.639373	50.220429
3503.572177	359727.063587	50.225434
3503.915195	359699.171145	50.230439
3503.874491	359716.404757	50.235444
3503.585196	359717.697387	50.240449
3504.141436	359694.427909	50.245453
3503.745819	359701.793568	50.250458
3503.783206	359722.959010	50.255463
3503.725027	359716.886574	50.260468
3503.876759	359693.986394	50.265473
3503.957214	359729.929329	50.270477
3503.537883	359700.757851	50.275482
3503.917805	359723.446817	50.280487
3504.186546	359720.503490	50.285492
3503.886108	359710.321602	50.290497
3503.858463	359717.221950	50.295501
3503.752422	359694.184394	50.300506
3503.675763	359738.167745	50.305511
3503.692214	359717.324664	50.310516
3503.884352	359725.208121	50.315521
3503.774854	359704.257712	50.320525
3503.763065	359735.024178	50.325530
3503.919646	359711.079942	50.330535
3504.083013	359732.937962	50.335540
3504.306117	359721.630019	50.340545
3504.180416	359718.927167	50.345549
3504.006387	359723.280579	50.350554
3503.888718	359694.544891	50.355559
3503.983519	359681.654103	50.360564
3503.540509	359698.442390	50.365569
3504.075669	359674.972664	50.370573
3503.635463	359684.991791	50.375578
3504.229910	359690.165242	50.380583
3503.884380	359688.438651	50.385588
3503.845688	359681.828758	50.390593
3504.033512	359693.097262	50.395597
3503.974621	359691.885180	50.400602
3504.021666	359676.991681	50.405607
3503.852416	359675.364456	50.410612
3503.822668	359677.888375	50.415617
3503.755818	359693.777474	50.420621
3503.674034	359676.207031	50.425626
3503.744965	359694.440856	50.430631
3504.002355	359697.351973	50.435636
3504.005590	359690.862684	50.440641
3504.116050	359688.275177	50.445645
3503.771702	359689.169370	50.450650
3503.937295	359655.350512	50.455655
3503.964823	359659.315820	50.460660
3503.906757	359651.182205	50.465665
3504.047624	359649.785867	50.470669
3503.534350	359674.728094	50.475674
3503.959992	359638.857858	50.480679
3503.856846	359680.122691	50.485684
3503.689578	359640.834589	50.490689
3503.632237	359673.822126	50.495693
3504.019452	359647.653017	50.500698
3504.120359	359669.622725	50.505703
3503.788498	359661.048912	50.510708
3503.669619	359663.765046	50.515713
3504.210625	359663.577772	50.520717
3503.531188	359666.789658	50.525722
3503.868069	359665.209657	50.530727
3503.889469	359664.595594	50.535732
3503.680002	359650.175223	50.540737
3503.754355	359607.769894	50.545741
3503.690771	359563.884996	50.550746
3503.725285	359530.799271	50.555751
3503.337517	359448.134301	50.560756
3503.268105	359413.080101	50.565761
3502.770747	359332.620653	50.570765
3502.616060	359237.093443	50.575770
3502.113421	359169.052474	50.580775
3501.965458	359062.709060	50.585780
3501.550771	358962.234870	50.590785
3501.785868	358862.802862	50.595789
3501.114468	358769.417604	50.600794
3500.937647	358638.114520	50.605799
3500.112241	358522.868833	50.610804
3499.831673	358393.744484	50.615809
3499.608570	358289.090772	50.620813
3499.303139	358132.105151	50.625818
3498.876255	358020.510570	50.630823
3498.212316	357859.763679	50.635828
3497.604558	357729.213373	50.640833
3497.521699	357552.596285	50.645837
3496.861977	357439.663043	50.650842
3496.558091	357245.062986	50.655847
3496.119685	357126.368344	50.660852
3495.488481	356929.910229	50.665857
3495.367331	356803.123184	50.670861
3494.085467	356606.384940	50.675866
3493.760555	356447.437605	50.680871
3493.552783	356259.714934	50.685876
3492.426842	356094.556543	50.690881
3492.085741	355918.559834	50.695885
3491.326864	355756.167070	50.700890
3490.912084	355564.530058	50.705895
3490.515619	355389.252825	50.710900
3489.859766	355218.851229	50.715905
3488.967079	355031.130502	50.720909
3488.479911	354823.800315	50.725914
3487.727982	354674.229205	50.730919
3487.489292	354462.175691	50.735924
3486.879120	354292.527273	50.740929
3486.120912	354093.889678	50.745933
3485.430549	353931.709358	50.750938
3485.118538	353704.114853	50.755943
3484.367278	353542.222890	50.760948
3483.486279	353331.818718	50.765953
3483.096919	353135.740467	50.770957
3482.258743	352931.664876	50.775962
3481.676599	352769.998294	50.780967
3481.241777	352564.686829	50.785972
3480.331698	352374.439742	50.790977
3479.889362	352164.139717	50.795981
3478.913940	351975.886640	50.800986
3478.360066	351787.795310	50.805991
3477.934818	351583.751061	50.810996
3477.046695	351393.038898	50.816001
3476.939599	351192.709535	50.821005
3476.309738	350993.760053	50.826010
3475.445782	350792.912591	50.831015
3474.870244	350586.012393	50.836020
3474.028305	350375.132276	50.841025
3473.306193	350196.911510	50.846029
3472.520821	349968.383325	50.851034
3472.285343	349795.632664	50.856039
3471.364910	349572.672543	50.861044
3470.643257	349385.592015	50.866049
3470.219367	349165.682272	50.871053
3469.058285	348975.361133	50.876058
3468.539672	348773.611781	50.881063
3468.070359	348585.368789	50.886068
3467.339270	348364.740893	50.891073
3466.861185	348178.457711	50.896077
3466.449517	347959.584811	50.901082
3465.418335	347758.345521	50.906087
3464.777744	347558.749063	50.911092
3463.770100	347357.148293	50.916097
3463.483382	347139.855964	50.921101
3462.593301	346954.804697	50.926106
3461.815127	346722.418788	50.931111
3461.106253	346552.609126	50.936116
3460.804569	346349.187862	50.941121
3460.283149	346139.157426	50.946125
3459.635424	345942.229006	50.951130
3458.984998	345724.199784	50.956135
3457.735144	345545.716845	50.961140
3457.123328	345333.457911	50.966145
3456.647856	345135.099602	50.971149
3456.118199	344929.393162	50.976154
3455.287183	344725.489935	50.981159
3454.572649	344523.374790	50.986164
3454.007582	344327.242384	50.991169
3453.330546	344117.458380	50.996173
3452.464982	343932.546364	51.001178
3452.037818	343724.019615	51.006183
3451.385482	343520.923983	51.011188
3450.548364	343317.500521	51.016193
3449.953685	343108.947212	51.021197
3449.228657	342912.708188	51.026202
3448.539802	342714.579190	51.031207
3447.802001	342517.551824	51.036212
3447.390751	342312.657665	51.041217
3446.765590	342109.374822	51.046221
3445.630270	341899.273748	51.051226
3445.284048	341710.505549	51.056231
3444.698316	341514.265467	51.061236
3444.038921	341309.967205	51.066241
3443.363787	341099.917931	51.071245
3442.779118	340900.824782	51.076250
3441.963866	340703.422038	51.081255
3441.164204	340491.226717	51.086260
3440.406914	340309.315807	51.091265
3439.963589	340099.531991	51.096269
3438.892362	339907.054655	51.101274
3438.386555	339691.806440	51.106279
3437.755539	339492.436159	51.111284
3436.546489	339310.415618	51.116289
3436.062490	339110.639066	51.121293
3435.407774	338913.816307	51.126298
3435.173399	338714.355439	51.131303
3434.538697	338531.936416	51.136308
3433.556269	338327.806895	51.141313
3433.003249	338102.887508	51.146317
3432.102359	337950.954534	51.151322
3431.792170	337717.111194	51.156327
3431.237473	337544.502905	51.161332
3430.419693	337329.016134	51.166337
3429.876744	337139.247252	51.171341
3428.748188	336946.235596	51.176346
3428.316600	336738.271921	51.181351
3427.557806	336554.365083	51.186356
3426.445067	336368.909919	51.191361
3426.035244	336148.136169	51.196365
3425.238755	335983.580997	51.201370
3424.816682	335775.078236	51.206375
3424.022720	335585.293726	51.211380
3423.164889	335401.603059	51.216385
3422.928835	335198.440591	51.221389
3421.980819	334996.484754	51.226394
3421.350716	334822.328497	51.231399
3420.662488	334600.219045	51.236404
3420.060509	334438.251520	51.241409
3419.721364	334225.046737	51.246413
3418.338772	334053.095048	51.251418
3417.878057	333861.623802	51.256423
3417.378709	333666.975909	51.261428
3416.736019	333468.480536	51.266433
3415.980096	333290.419820	51.271437
3415.352085	333079.141117	51.276442
3414.787039	332916.044081	51.281447
3414.056533	332690.676625	51.286452
3413.506272	332511.486736	51.291457
3412.977443	332311.162590	51.296461
3412.128835	332102.919962	51.301466
3411.414445	331931.875815	51.306471
3410.818691	331743.551615	51.311476
3410.177177	331544.592463	51.316481
3409.518792	331340.976497	51.321485
3408.648777	331159.542539	51.326490
3408.121550	330957.457752	51.331495
3407.533495	330778.906036	51.336500
3406.708938	330589.698527	51.341505
3406.564687	330369.042924	51.346509
3405.257523	330193.862257	51.351514
3404.647225	329998.661944	51.356519
3404.163288	329797.763738	51.361524
3403.325352	329609.345097	51.366529
3402.738261	329432.521241	51.371533
3402.095861	329229.940805	51.376538
3401.571344	329033.247786	51.381543
3401.108314	328833.438476	51.386548
3400.161894	328652.010529	51.391553
3399.752080	328448.398321	51.396557
3398.910383	328246.839724	51.401562
3398.407105	328048.842383	51.406567
3397.553239	327867.627099	51.411572
3396.741922	327653.434071	51.416577
3396.213625	327492.101555	51.421581
3395.510865	327279.036039	51.426586
3395.025282	327101.477918	51.431591
3394.246865	326875.871447	51.436596
3393.267179	326724.156302	51.441601
3393.064466	326492.016276	51.446605
3392.075382	326312.371886	51.451610
3391.515442	326127.872679	51.456615
3391.233126	325942.056128	51.461620
3390.154291	325720.873114	51.466625
3389.674867	325536.538054	51.471629
3388.940995	325342.975132	51.476634
3388.462221	325136.259146	51.481639
3387.599199	324956.439063	51.486644
3386.788146	324755.808868	51.491649
3386.048261	324557.534799	51.496653
3385.193296	324371.830707	51.501658
3384.367579	324183.371788	51.506663
3384.058069	323994.092449	51.511668
3383.175298	323800.804091	51.516673
3382.586204	323620.886898	51.521677
3381.507498	323444.331244	51.526682
3381.300372	323241.590501	51.531687
3380.387736	323057.700396	51.536692
3379.831583	322864.409190	51.541697
3379.100038	322691.972762	51.546701
3378.498290	322495.377952	51.551706
3378.091908	322306.848584	51.556711
3377.527644	322131.532896	51.561716
3376.863451	321938.282178	51.566721
3376.129261	321741.553846	51.571725
3374.947420	321569.008177	51.576730
3374.608949	321376.443115	51.581735
3374.118008	321191.413006	51.586740
3373.080337	321008.200381	51.591745
3372.744630	320822.788497	51.596749
3372.051163	320629.870575	51.601754
3371.236079	320442.445826	51.606759
3370.318759	320253.814674	51.611764
3370.034012	320062.969739	51.616769
3369.447030	319866.112181	51.621773
3368.428488	319682.308228	51.626778
3368.127406	319482.858411	51.631783
3367.712134	319302.828589	51.636788
3366.878227	319121.311410	51.641793
3366.274238	318923.181420	51.646797
3365.565476	318734.616046	51.651802
3364.537073	318540.626378	51.656807
3364.242524	318352.071131	51.661812
3363.353450	318159.128085	51.666817
3362.736473	317960.565274	51.671821
3361.764209	317777.234084	51.676826
3361.463932	317589.187500	51.681831
3360.545464	317403.046179	51.686836
3359.764635	317220.498479	51.691841
3358.984861	317026.288207	51.696845
3358.558501	316845.491630	51.701850
3358.329552	316657.024569	51.706855
3357.886312	316476.000819	51.711860
3356.620454	316290.039648	51.716865
3356.018031	316086.479956	51.721869
3355.488959	315899.561261	51.726874
3354.462787	315715.547264	51.731879
3353.974513	315525.362117	51.736884
3353.313730	315343.530446	51.741889
3352.566721	315154.505918	51.746893
3351.888199	314976.903344	51.751898
3350.972940	314783.499552	51.756903
3350.426587	314604.551333	51.761908
3349.597215	314427.684659	51.766913
3349.499551	314233.564890	51.771917
3348.400537	314055.517973	51.776922
3347.991443	313861.217597	51.781927
3347.142782	313679.616453	51.786932
3346.238648	313492.701819	51.791937
3346.182606	313309.166765	51.796941
3345.595339	313136.232035	51.801946
3344.858347	312928.333133	51.806951
3343.796707	312747.222457	51.811956
3343.195652	312559.952720	51.816961
3342.647331	312385.304548	51.821965
3341.820324	312193.613696	51.826970
3340.982971	312006.278536	51.831975
3340.425922	311831.656341	51.836980
3339.553711	311651.838066	51.841985
3339.119085	311470.473370	51.846989
3338.188928	311281.547428	51.851994
3337.340092	311104.729391	51.856999
3336.885537	310936.583046	51.862004
3336.193456	310757.014984	51.867009
3335.888366	310565.060595	51.872013
3334.948502	310402.210461	51.877018
3334.411147	310211.641846	51.882023
3334.000583	310026.578708	51.887028
3332.963196	309846.630961	51.892033
3332.537353	309674.658557	51.897037
3331.415743	309489.554245	51.902042
3331.172134	309312.714190	51.907047
3330.805447	309136.708217	51.912052
3329.656203	308941.268699	51.917057
3329.091498	308772.041717	51.922061
3328.154025	308594.953846	51.927066
3327.811325	308410.310406	51.932071
3327.513544	308220.541111	51.937076
3326.448281	308041.384526	51.942081
3326.328927	307848.097731	51.947085
3325.271123	307677.164686	51.952090
3324.674281	307481.151677	51.957095
3323.822087	307305.168971	51.962100
3323.168436	307126.022394	51.967105
3322.799185	306937.586681	51.972109
3321.956772	306746.806318	51.977114
3321.085395	306568.457368	51.982119
3320.866637	306385.472118	51.987124
3319.822023	306204.068757	51.992129
3319.319114	306025.609871	51.997133
3318.597093	305846.268641	52.002138
3317.848247	305662.271217	52.007143
3317.275718	305475.418978	52.012148
3316.244632	305291.185568	52.017153
3316.201941	305101.957115	52.022157
3315.521026	304927.064668	52.027162
3314.532153	304738.672936	52.032167
3314.097030	304556.967266	52.037172
3313.371763	304374.415946	52.042177
3312.845340	304198.912444	52.047181
3312.099606	304010.888741	52.052186
3311.316111	303823.456479	52.057191
3310.860669	303637.321784	52.062196
3310.118810	303459.177530	52.067201
3309.190246	303270.086745	52.072205
3308.341183	303095.829836	52.077210
3307.838307	302914.260144	52.082215
3307.028546	302739.614611	52.087220
3306.404872	302553.581556	52.092225
3305.955648	302371.900859	52.097229
3304.921552	302188.606214	52.102234
3304.334524	302004.323858	52.107239
3303.993551	301842.361722	52.112244
3303.047096	301653.399076	52.117249
3302.415731	301463.953440	52.122253
3301.686148	301280.507697	52.127258
3300.775893	301123.549857	52.132263
3300.567414	300952.754493	52.137268
3299.676613	300773.255487	52.142273
3299.004140	300585.725291	52.147277
3298.383014	300413.517570	52.152282
3297.621743	300228.420323	52.157287
3297.119397	300051.787734	52.162292
3296.317995	299874.030796	52.167297
3295.663209	299696.225014	52.172301
3295.056632	299524.650737	52.177306
3294.506628	299354.187870	52.182311
3293.831460	299171.418773	52.187316
3293.016595	298991.447445	52.192321
3292.255549	298814.243289	52.197325
3291.663327	298651.146286	52.202330
3291.240043	298466.121007	52.207335
3290.775479	298283.877943	52.212340
3289.839644	298114.850104	52.217345
3289.524669	297938.109327	52.222349
3288.586324	297755.915201	52.227354
3287.799473	297566.897276	52.232359
3287.331099	297391.708249	52.237364
3286.499613	297219.377852	52.242369
3285.922023	297043.594568	52.247373
3284.870970	296868.650017	52.252378
3284.198017	296684.502851	52.257383
3283.644017	296501.304442	52.262388
3282.904233	296338.534348	52.267393
3282.345361	296163.358511	52.272397
3281.600102	295988.135599	52.277402
3281.122807	295812.666413	52.282407
3280.486109	295634.013428	52.287412
3279.801142	295462.447789	52.292417
3279.425826	295285.968799	52.297421
3278.686811	295105.090425	52.302426
3278.001451	294932.251049	52.307431
3277.564520	294754.151452	52.312436
3276.450529	294569.002497	52.317441
3276.116634	294390.173217	52.322445
3275.058194	294205.167967	52.327450
3274.503256	294039.820098	52.332455
3274.093484	293852.674565	52.337460
3273.215566	293669.066484	52.342465
3272.822821	293492.614251	52.347469
3271.815628	293320.588528	52.352474
3271.076439	293138.791729	52.357479
3270.781215	292965.558029	52.362484
3270.118459	292771.753688	52.367489
3269.191681	292600.580609	52.372493
3268.476052	292424.000366	52.377498
3267.614267	292251.237774	52.382503
3267.025006	292069.390977	52.387508
3266.601518	291906.847700	52.392513
3266.243902	291733.190037	52.397517
3265.037724	291549.504906	52.402522
3264.265985	291375.581423	52.407527
3264.040497	291198.617175	52.412532
3263.213080	291022.894061	52.417537
3262.392911	290845.004932	52.422541
3261.704224	290662.892721	52.427546
3261.187827	290498.376779	52.432551
3260.746438	290322.108260	52.437556
3259.702653	290141.528996	52.442561
3259.481781	289968.281499	52.447565
3258.632981	289796.075527	52.452570
3258.011480	289609.062189	52.457575
3257.243196	289435.009585	52.462580
3256.255531	289259.387108	52.467585
3255.597245	289084.731140	52.472589
3255.136717	288914.857210	52.477594
3254.386790	288738.178112	52.482599
3253.560746	288584.381093	52.487604
3253.026850	288409.959743	52.492609
3252.563769	288224.474033	52.497613
3251.938335	288049.761352	52.502618
3251.300469	287876.909702	52.507623
3250.876482	287700.127537	52.512628
3249.991468	287527.544012	52.517633
3249.502101	287339.769849	52.522637
3248.560170	287176.083467	52.527642
3247.679771	286999.678753	52.532647
3246.866323	286819.952522	52.537652
3246.287471	286652.693885	52.542657
3245.515209	286473.470328	52.547661
3244.951492	286312.219595	52.552666
3244.384026	286150.994855	52.557671
3243.904171	285979.034138	52.562676
3242.737150	285804.915387	52.567681
3242.158768	285635.720658	52.572685
3241.216223	285479.342972	52.577690
3240.873225	285306.316127	52.582695
3240.264967	285139.010558	52.587700
3239.294645	284978.205629	52.592705
3239.055469	284798.183891	52.597709
3238.443911	284637.780512	52.602714
3237.513337	284470.856759	52.607719
3237.037291	284293.801124	52.612724
3236.319950	284120.756625	52.617729
3235.809121	283950.506363	52.622733
3234.730197	283780.116693	52.627738
3234.314181	283617.771921	52.632743
3233.795714	283452.820079	52.637748
3232.890624	283290.730846	52.642753
3232.506291	283112.463275	52.647757
3231.566979	282950.048265	52.652762
3231.082600	282784.403183	52.657767
3230.415031	282608.319585	52.662772
3229.990710	282438.462642	52.667777
3229.077878	282270.542110	52.672781
3228.290855	282110.089297	52.677786
3227.940634	281934.872157	52.682791
3227.254647	281757.797964	52.687796
3226.921456	281597.655255	52.692801
3225.884450	281407.265650	52.697805
3225.317390	281232.999486	52.702810
3224.364668	281067.096952	52.707815
3223.644560	280903.398795	52.712820
3222.930427	280736.312372	52.717825
3222.534569	280567.392783	52.722829
3221.705072	280397.166468	52.727834
3220.979283	280233.927502	52.732839
3220.536501	280058.775494	52.737844
3219.443362	279891.901670	52.742849
3219.369523	279726.165454	52.747853
3218.410433	279549.235840	52.752858
3217.877806	279379.446273	52.757863
3217.126112	279222.170825	52.762868
3216.463641	279054.210001	52.767873
3215.783779	278879.910282	52.772877
3215.104343	278708.743079	52.777882
3214.534940	278535.597383	52.782887
3213.878245	278357.651953	52.787892
3213.063718	278207.593867	52.792897
3212.489139	278015.271244	52.797901
3211.710481	277864.952768	52.802906
3210.921083	277695.076264	52.807911
3210.609306	277527.721960	52.812916
3209.593338	277350.317160	52.817921
3208.967591	277187.138377	52.822925
3208.260971	277028.302004	52.827930
3207.362750	276868.680944	52.832935
3206.948508	276688.099232	52.837940
3206.264813	276538.555168	52.842945
3205.643157	276352.861638	52.847949
3205.173542	276202.748860	52.852954
3204.573493	276026.449737	52.857959
3203.948851	275861.640746	52.862964
3202.989798	275705.594848	52.867969
3202.842353	275531.337992	52.872973
3201.767569	275360.793418	52.877978
3200.981945	275198.505795	52.882983
3200.817862	275029.345253	52.887988
3199.999736	274864.133913	52.892993
3199.243907	274689.413013	52.897997
3198.517472	274525.486065	52.903002
3197.945683	274362.375116	52.908007
3197.303441	274180.912613	52.913012
3196.431920	274036.288211	52.918017
3196.014608	273849.110695	52.923021
3195.072509	273690.107842	52.928026
3194.621089	273509.353781	52.933031
3194.021252	273352.308808	52.938036
3193.392182	273170.411338	52.943041
3192.493998	273008.396326	52.948045
3192.045038	272836.504937	52.953050
3191.073034	272676.972070	52.958055
3190.241949	272507.611606	52.963060
3189.404299	272350.094991	52.968065
3189.021337	272176.919824	52.973069
3188.225810	272028.514258	52.978074
3187.423364	271858.538111	52.983079
3187.138110	271700.144669	52.988084
3186.281501	271526.127676	52.993089
3185.960252	271379.531821	52.998093
3185.001660	271207.925042	53.003098
3184.089297	271044.231632	53.008103
3183.584129	270870.184625	53.013108
3182.974116	270718.591831	53.018113
3182.515939	270558.213942	53.023117
3181.946841	270396.809432	53.028122
3181.084333	270236.189956	53.033127
3180.696306	270061.309602	53.038132
3179.798577	269911.952756	53.043137
3179.300456	269727.259138	53.048141
3178.468571	269572.441732	53.053146
3177.867730	269403.223700	53.058151
3177.343560	269240.411584	53.063156
3176.436602	269078.678802	53.068161
3176.009273	268902.404207	53.073165
3174.890430	268746.817415	53.078170
3174.222711	268579.647645	53.083175
3173.950226	268413.281310	53.088180
3173.013758	268251.044055	53.093185
3172.414674	268101.207428	53.098189
3171.772575	267934.212072	53.103194
3171.109585	267771.218581	53.108199
3170.641348	267603.533647	53.113204
3169.680386	267444.509505	53.118209
3169.256355	267273.965248	53.123213
3168.495991	267125.911724	53.128218
3167.415060	266950.072259	53.133223
3167.091661	266782.313752	53.138228
3166.198742	266637.770490	53.143233
3165.583133	266470.287542	53.148237
3165.182016	266321.617135	53.153242
3164.358746	266162.698981	53.158247
3164.176722	265993.186568	53.163252
3163.013723	265834.908052	53.168257
3162.295490	265666.448394	53.173261
3161.929730	265511.991418	53.178266
3160.969828	265342.042045	53.183271
3160.602046	265179.970562	53.188276
3159.797749	265012.467113	53.193281
3158.997727	264857.977227	53.198285
3158.410815	264708.037930	53.203290
3157.512780	264558.147919	53.208295
3157.173418	264384.458861	53.213300
3156.229857	264236.944708	53.218305
3155.922785	264069.643158	53.223309
3155.190114	263908.674146	53.228314
3154.258612	263751.709669	53.233319
3153.860784	263584.295369	53.238324
3153.042565	263437.958715	53.243329
3152.259023	263253.542089	53.248333
3151.729967	263119.690041	53.253338
3151.224732	262945.977011	53.258343
3150.717560	262789.658948	53.263348
3149.755184	262628.625025	53.268353
3149.241687	262463.674513	53.273357
3148.651624	262306.020008	53.278362
3147.715499	262148.598613	53.283367
3147.292913	261974.745704	53.288372
3146.299650	261831.646431	53.293377
3145.598401	261670.291549	53.298381
3144.860779	261511.896773	53.303386
3144.271343	261349.556600	53.308391
3143.692876	261198.879015	53.313396
3142.726540	261047.702589	53.318401
3142.256683	260874.494510	53.323405
3141.867683	260729.593838	53.328410
3141.198532	260579.975110	53.333415
3140.419075	260402.690547	53.338420
3139.751121	260257.554119	53.343425
3139.363017	260090.573180	53.348429
3138.648810	259940.121505	53.353434
3138.066009	259775.947544	53.358439
3137.353960	259614.697445	53.363444
3136.330779	259456.731061	53.368449
3135.737369	259296.710303	53.373453
3135.233734	259126.972302	53.378458
3134.329263	258985.846954	53.383463
3133.792943	258824.798764	53.388468
3132.894510	258667.628103	53.393473
3132.230907	258507.797236	53.398477
3131.756829	258356.137014	53.403482
3131.095207	258202.112623	53.408487
3130.788618	258041.741697	53.413492
3129.612744	257890.269222	53.418497
3128.980213	257719.202840	53.423501
3128.461485	257560.444794	53.428506
3127.856281	257408.933275	53.433511
3127.195477	257254.960322	53.438516
3126.430454	257099.934339	53.443521
3126.150271	256937.904636	53.448525
3125.307478	256791.397259	53.453530
3124.465282	256620.746904	53.458535
3123.741004	256459.933854	53.463540
3122.583932	256305.836359	53.468545
3122.230035	256146.187367	53.473549
3121.760742	256000.538252	53.478554
3121.046171	255841.379506	53.483559
3120.659703	255694.647877	53.488564
3119.771872	255537.274015	53.493569
3119.204036	255366.912340	53.498573
3118.487083	255214.528713	53.503578
3117.752034	255068.209234	53.508583
3117.241518	254911.540169	53.513588
3116.607242	254754.534272	53.518593
3115.838748	254598.593888	53.523597
3115.050667	254452.232323	53.528602
3114.251045	254285.040698	53.533607
3113.468477	254133.483237	53.538612
3112.674381	253980.552506	53.543617
3112.419647	253837.825190	53.548621
3111.367230	253686.157987	53.553626
3110.651586	253535.634560	53.558631
3110.469454	253385.943640	53.563636
3109.416517	253244.514561	53.568641
3108.661540	253080.729503	53.573645
3108.086813	252936.601909	53.578650
3107.492296	252779.744169	53.583655
3107.263621	252636.504326	53.588660
3106.348417	252496.887646	53.593665
3105.828970	252343.150820	53.598669
3105.411865	252187.640732	53.603674
3104.253646	252021.730321	53.608679
3104.048379	251873.190327	53.613684
3103.082178	251716.647018	53.618689
3102.444283	251565.247088	53.623693
3101.497959	251416.926622	53.628698
3100.916830	251265.594376	53.633703
3100.159431	251102.422753	53.638708
3099.355855	250970.276810	53.643713
3099.097512	250819.250421	53.648717
3098.384649	250672.166997	53.653722
3097.480870	250523.509531	53.658727
3097.005674	250359.326261	53.663732
3096.412178	250221.112136	53.668737
3096.063256	250064.116175	53.673741
3095.154619	249919.076258	53.678746
3094.437180	249763.259427	53.683751
3093.970055	249608.854718	53.688756
3092.991860	249461.814390	53.693761
3092.164099	249305.455213	53.698765
3091.856233	249158.512824	53.703770
3090.856035	249007.147149	53.708775
3090.667831	248854.787278	53.713780
3089.669537	248714.372048	53.718785
3089.162819	248547.750909	53.723789
3088.305148	248400.947185	53.728794
3088.017408	248250.539095	53.733799
3087.183176	248104.037545	53.738804
3086.496248	247957.971217	53.743809
3086.103623	247795.636619	53.748813
3085.140861	247643.527879	53.753818
3084.627227	247501.865660	53.758823
3084.113108	247338.328429	53.763828
3083.264057	247181.032597	53.768833
3082.568609	247020.274738	53.773837
3081.545069	246874.873948	53.778842
3080.786584	246734.269865	53.783847
3080.211039	246591.599708	53.788852
3079.754741	246444.123262	53.793857
3078.913647	246298.057549	53.798861
3078.463943	246148.135661	53.803866
3077.772270	246004.313058	53.808871
3077.245689	245852.799318	53.813876
3076.273317	245694.633367	53.818881
3075.722517	245552.189553	53.823885
3075.317952	245401.726557	53.828890
3074.327718	245247.409254	53.833895
3074.301511	245087.693672	53.838900
3073.037742	244955.294866	53.843905
3072.587491	244796.818150	53.848909
3071.976991	244643.740187	53.853914
3071.117112	244501.728383	53.858919
3070.286847	244353.167447	53.863924
3069.357469	244205.309928	53.868929
3068.955285	244067.606201	53.873933
3068.374321	243914.397091	53.878938
3067.852219	243767.468764	53.883943
3067.511038	243610.198558	53.888948
3066.301818	243467.479216	53.893953
3065.778214	243320.959083	53.898957
3065.357144	243169.813704	53.903962
3064.220019	243029.680890	53.908967
3063.831828	242866.409282	53.913972
3063.121169	242747.090654	53.918977
3062.312175	242580.830210	53.923981
3061.985866	242434.967444	53.928986
3061.253599	242289.372817	53.933991
3060.541269	242130.533449	53.938996
3059.581391	241997.605791	53.944001
3059.177775	241857.103576	53.949005
3058.512819	241701.236659	53.954010
3057.552113	241557.028698	53.959015
3057.147815	241417.571158	53.964020
3056.448364	241269.400622	53.969025
3055.948590	241114.475987	53.974029
3055.132062	240974.778629	53.979034
3053.967947	240841.146103	53.984039
3053.999114	240688.098777	53.989044
3053.430838	240540.901515	53.994049
3052.672910	240385.916837	53.999053
3051.879168	240246.267671	54.004058
3051.381568	240102.522953	54.009063
3050.807878	239952.246093	54.014068
3050.070321	239799.703566	54.019073
3049.434717	239645.286207	54.024077
3048.461617	239511.803239	54.029082
3047.569175	239353.454486	54.034087
3047.246582	239195.754234	54.039092
3046.577712	239067.902178	54.044097
3046.024237	238919.686092	54.049101
3045.436773	238768.343488	54.054106
3044.644280	238618.714173	54.059111
3044.145816	238469.420487	54.064116
3043.227938	238317.010373	54.069121
3042.669490	238163.168526	54.074125
3041.920757	238020.102824	54.079130
3041.162215	237878.719486	54.084135
3040.723008	237728.831763	54.089140
3039.790542	237580.983035	54.094145
3039.425806	237438.824956	54.099149
3038.831616	237283.283938	54.104154
3037.963388	237137.335444	54.109159
3037.508588	236993.511602	54.114164
3036.454204	236841.430747	54.119169
3036.011805	236692.639923	54.124173
3035.241992	236557.091307	54.129178
3034.491247	236403.333355	54.134183
3034.054816	236249.907837	54.139188
3033.338294	236112.747158	54.144193
3032.648526	235967.077611	54.149197
3031.746745	235820.550604	54.154202
3031.247006	235668.256362	54.159207
3030.800557	235513.076547	54.164212
3030.000294	235379.138491	54.169217
3029.269394	235236.175612	54.174221
3028.533598	235090.590989	54.179226
3027.981691	234952.692842	54.184231
3027.669227	234794.182698	54.189236
3026.668223	234651.136083	54.194241
3025.923786	234502.345320	54.199245
3025.448828	234360.259854	54.204250
3024.659132	234212.877159	54.209255
3024.194619	234067.531186	54.214260
3023.450547	233913.190310	54.219265
3022.586545	233766.660323	54.224269
3022.150870	233619.069710	54.229274
3021.544541	233490.221552	54.234279
3020.948143	233326.869830	54.239284
3019.826393	233179.770417	54.244289
3019.319777	233051.161690	54.249293
3018.725507	232890.254798	54.254298
3017.884392	232744.257457	54.259303
3017.177438	232599.028447	54.264308
3016.461136	232456.041850	54.269313
3015.953040	232307.726298	54.274317
3015.315596	232164.549421	54.279322
3014.054616	232030.103242	54.284327
3014.122355	231879.431060	54.289332
3013.119050	231750.087916	54.294337
3012.802204	231598.916884	54.299341
3012.167683	231455.104072	54.304346
3011.091934	231310.622914	54.309351
3010.704399	231159.845722	54.314356
3009.973948	231029.569219	54.319361
3009.474769	230875.321841	54.324365
3008.817495	230723.951506	54.329370
3007.685425	230588.264841	54.334375
3007.290180	230439.145095	54.339380
3006.801885	230306.717946	54.344385
3006.093933	230159.965201	54.349389
3005.243791	230026.526335	54.354394
3004.367126	229876.159700	54.359399
3004.007294	229719.855285	54.364404
3002.795178	229593.781913	54.369409
3002.297728	229451.401908	54.374413
3001.957783	229317.705116	54.379418
3001.015948	229173.842730	54.384423
3000.942147	229036.132214	54.389428
3000.127026	228899.277639	54.394433
2999.190666	228750.908374	54.399437
2998.726426	228615.984708	54.404442
2998.188126	228473.383601	54.409447
2997.905689	228326.642935	54.414452
2996.747467	228185.540807	54.419457
2996.192890	228042.510143	54.424461
2996.103314	227896.070680	54.429466
2994.951560	227765.280057	54.434471
2994.331549	227598.377808	54.439476
2993.386150	227455.613677	54.444481
2992.894404	227306.539998	54.449485
2992.028690	227169.848951	54.454490
2991.240535	227033.655071	54.459495
2990.947438	226884.894418	54.464500
2989.733280	226757.717966	54.469505
2988.909979	226610.149278	54.474509
2988.902490	226458.607123	54.479514
2987.952699	226321.306979	54.484519
2987.382700	226184.761692	54.489524
2986.733280	226048.674765	54.494529
2986.039860	225901.430500	54.499533
2985.464668	225760.214695	54.504538
2984.401524	225629.006020	54.509543
2983.636690	225481.404635	54.514548
2982.973567	225347.281507	54.519553
2982.457541	225210.589266	54.524557
2982.003409	225074.893146	54.529562
2981.160848	224955.960777	54.534567
2980.628885	224800.749293	54.539572
2980.007782	224668.886613	54.544577
2979.305336	224525.338022	54.549581
2978.736707	224376.740108	54.554586
2977.892168	224252.055082	54.559591
2977.266995	224118.220790	54.564596
2976.565565	223973.158153	54.569601
2975.976848	223823.011388	54.574605
2975.818435	223693.050240	54.579610
2974.465986	223578.567035	54.584615
2974.101517	223426.310540	54.589620
2973.146907	223292.096980	54.594625
2972.698050	223151.604120	54.599629
2972.234557	223008.185953	54.604634
2971.600893	222878.479606	54.609639
2970.946615	222722.273181	54.614644
2970.170037	222590.718651	54.619649
2969.491672	222446.546288	54.624653
2968.726648	222295.615669	54.629658
2968.094060	222166.190407	54.634663
2967.657057	222029.733047	54.639668
2966.803755	221893.341830	54.644673
2966.222304	221749.206360	54.649677
2965.546650	221600.961664	54.654682
2964.711235	221471.378747	54.659687
2964.281668	221322.420971	54.664692
2963.635563	221185.272644	54.669697
2962.911630	221056.232897	54.674701
2962.528647	220917.655883	54.679706
2961.464143	220773.751503	54.684711
2961.210559	220634.912670	54.689716
2960.451718	220488.503662	54.694721
2959.741370	220352.716360	54.699725
2959.191650	220207.624126	54.704730
2958.206619	220077.010774	54.709735
2957.930397	219925.421992	54.714740
2956.997157	219783.497274	54.719745
2956.283350	219631.647406	54.724749
2955.659643	219489.496050	54.729754
2954.874237	219362.683895	54.734759
2954.524493	219217.714718	54.739764
2953.646257	219075.948154	54.744769
2952.757513	218938.816964	54.749773
2952.373908	218803.120843	54.754778
2951.264382	218659.800564	54.759783
2950.691393	218524.300429	54.764788
2949.912653	218393.084645	54.769793
2949.144672	218258.125047	54.774797
2948.558570	218114.901210	54.779802
2947.903173	217985.690572	54.784807
2947.540869	217850.374760	54.789812
2947.058945	217714.339862	54.794817
2946.342959	217571.532283	54.799821
2945.887183	217433.533527	54.804826
2944.611722	217307.680900	54.809831
2944.415011	217147.366095	54.814836
2943.958691	217015.223538	54.819841
2942.821064	216870.676639	54.824845
2942.167206	216742.320878	54.829850
2941.513512	216613.723482	54.834855
2941.294059	216478.464081	54.839860
2940.504551	216336.052536	54.844865
2939.817960	216192.059361	54.849869
2939.051331	216055.780014	54.854874
2938.200809	215916.115666	54.859879
2937.570911	215764.044444	54.864884
2936.945229	215634.451613	54.869889
2936.352113	215495.676564	54.874893
2935.619186	215357.305789	54.879898
2934.821097	215222.305945	54.884903
2934.102360	215088.172075	54.889908
2933.609889	214961.932495	54.894913
2933.225240	214826.040640	54.899917
2932.583565	214666.133020	54.904922
2931.413244	214541.796250	54.909927
2930.714863	214399.437985	54.914932
2930.217482	214261.210374	54.919937
2929.552566	214120.858486	54.924941
2929.053447	213992.801638	54.929946
2928.352200	213859.825739	54.934951
2927.736015	213715.292122	54.939956
2926.797405	213591.900524	54.944961
2926.211936	213452.912125	54.949965
2925.517991	213324.581941	54.954970
2924.697381	213196.832099	54.959975
2924.281320	213044.593205	54.964980
2923.689211	212916.311340	54.969985
2922.925222	212776.818060	54.974989
2922.366659	212647.907739	54.979994
2921.479742	212514.009365	54.984999
2920.830324	212367.816622	54.990004
2919.966677	212250.117834	54.995009
2919.265250	212107.459559	55.000013
2918.919115	211977.906004	55.005018
2917.929679	211853.838449	55.010023
2917.346815	211719.753585	55.015028
2917.096948	211584.241678	55.020033
2916.000318	211456.373519	55.025037
2915.652189	211324.212405	55.030042
2914.812039	211198.569703	55.035047
2914.410119	211053.193539	55.040052
2913.736777	210927.626788	55.045057
2912.764469	210788.336282	55.050061
2912.262196	210652.624500	55.055066
2911.809751	210526.730840	55.060071
2911.001648	210395.229964	55.065076
2910.237002	210255.602302	55.070081
2909.509840	210121.289124	55.075085
2908.916277	209991.562442	55.080090
2908.156405	209879.222643	55.085095
2907.832211	209724.635286	55.090100
2906.676602	209597.811177	55.095105
2906.134240	209472.073886	55.100109
2905.837776	209333.188728	55.105114
2904.978913	209212.796661	55.110119
2904.243792	209079.301556	55.115124
2903.440336	208939.581188	55.120129
2902.998618	208808.152951	55.125133
2902.491481	208675.488084	55.130138
2901.570738	208541.628996	55.135143
2900.868353	208401.219317	55.140148
2900.429679	208278.993488	55.145153
2899.834577	208148.532768	55.150157
2899.221419	208008.428050	55.155162
2897.965484	207883.201549	55.160167
2897.355434	207753.456765	55.165172
2896.712779	207634.229937	55.170177
2896.068063	207498.687673	55.175181
2895.291026	207373.590045	55.180186
2894.375559	207248.756407	55.185191
2894.021459	207111.323604	55.190196
2893.603462	206998.578648	55.195201
2892.859442	206866.757064	55.200205
2892.177240	206737.242267	55.205210
2891.347817	206618.174309	55.210215
2890.872361	206487.761902	55.215220
2890.105450	206366.190107	55.220225
2889.638854	206233.651493	55.225229
2889.143756	206104.159367	55.230234
2888.174879	205983.803922	55.235239
2887.880623	205844.162877	55.240244
2887.089448	205719.872764	55.245249
2886.224622	205593.036535	55.250253
2885.866344	205463.231454	55.255258
2884.726170	205330.267019	55.260263
2884.393641	205187.795591	55.265268
2883.618844	205072.590981	55.270273
2883.090465	204953.427843	55.275277
2882.381545	204817.443772	55.280282
2881.382675	204691.814296	55.285287
2881.063491	204554.852838	55.290292
2880.525330	204428.578306	55.295297
2879.930199	204300.200509	55.300301
2879.561288	204163.960530	55.305306
2878.953259	204035.063592	55.310311
2878.065889	203902.965994	55.315316
2876.986925	203768.302899	55.320321
2876.341541	203636.447581	55.325325
2875.619240	203496.969081	55.330330
2874.654723	203373.933197	55.335335
2874.152258	203252.567892	55.340340
2873.733965	203123.452095	55.345345
2873.031050	202999.777483	55.350349
2872.497125	202869.649771	55.355354
2871.752607	202737.532280	55.360359
2871.270891	202611.087425	55.365364
2870.538359	202492.801683	55.370369
2869.865715	202347.120669	55.375373
2869.340409	202225.277622	55.380378
2868.452511	202082.800113	55.385383
2868.006376	201957.649138	55.390388
2867.203130	201826.764781	55.395393
2866.110155	201699.680691	55.400397
2865.642580	201587.590521	55.405402
2865.077132	201444.452769	55.410407
2864.497664	201323.816495	55.415412
2863.623748	201197.831459	55.420417
2862.700151	201071.256478	55.425421
2862.544363	200933.247221	55.430426
2861.470976	200824.830406	55.435431
2861.082273	200681.679386	55.440436
2860.470408	200561.877078	55.445441
2859.813709	200430.374756	55.450445
2859.228226	200311.994067	55.455450
2858.733506	200182.133724	55.460455
2858.197301	200048.666270	55.465460
2857.281533	199917.817030	55.470465
2856.385686	199793.162154	55.475469
2855.975281	199662.857051	55.480474
2855.225415	199535.863665	55.485479
2854.605508	199403.212754	55.490484
2854.031400	199270.771246	55.495489
2853.280686	199150.726833	55.500493
2852.609881	199022.475087	55.505498
2851.857669	198897.188751	55.510503
2851.187731	198761.366096	55.515508
2850.658801	198628.842681	55.520513
2850.033214	198497.938246	55.525517
2849.313548	198367.252630	55.530522
2848.502544	198248.314148	55.535527
2847.932005	198123.051777	55.540532
2847.162159	197992.553184	55.545537
2846.664159	197864.607728	55.550541
2845.799554	197740.385368	55.555546
2844.877045	197609.861002	55.560551
2844.336448	197478.131264	55.565556
2843.660184	197377.038910	55.570561
2843.076148	197238.407155	55.575565
2842.710285	197111.536939	55.580570
2841.540102	196989.540664	55.585575
2841.273222	196859.410621	55.590580
2840.716372	196736.032643	55.595585
2839.890112	196610.203620	55.600589
2839.442450	196479.390588	55.605594
2838.533682	196359.466667	55.610599
2837.928347	196221.171844	55.615604
2837.488646	196098.998383	55.620609
2836.260762	195974.850506	55.625613
2835.976464	195839.788754	55.630618
2835.365546	195725.646880	55.635623
2834.859688	195590.251868	55.640628
2834.010617	195467.699390	55.645633
2833.173874	195338.388718	55.650637
2833.075075	195220.693182	55.655642
2832.100393	195090.374328	55.660647
2831.155837	194947.021583	55.665652
2830.805007	194835.677994	55.670657
2829.867531	194702.300478	55.675661
2829.491279	194570.552181	55.680666
2828.445452	194444.636036	55.685671
2827.849149	194324.082138	55.690676
2827.279266	194187.950306	55.695681
2826.416781	194075.773301	55.700685
2826.013659	193955.291489	55.705690
2825.236999	193839.093420	55.710695
2824.980530	193700.152222	55.715700
2823.699095	193573.957487	55.720705
2823.077759	193462.532547	55.725709
2822.684719	193319.898718	55.730714
2821.896099	193206.808595	55.735719
2821.253904	193071.212937	55.740724
2820.705026	192967.246391	55.745729
2820.028248	192831.402396	55.750733
2819.419868	192706.019390	55.755738
2818.552086	192587.535734	55.760743
2818.283326	192454.707247	55.765748
2817.663900	192329.148824	55.770753
2816.639248	192208.286202	55.775757
2816.389643	192075.277584	55.780762
2815.462800	191947.898490	55.785767
2814.917071	191815.382789	55.790772
2814.096670	191695.990440	55.795777
2813.302243	191566.084898	55.800781
2812.616588	191441.875185	55.805786
2811.794859	191327.026129	55.810791
2811.586516	191192.944645	55.815796
2810.688683	191089.991592	55.820801
2809.989455	190955.657704	55.825805
2809.359418	190826.186148	55.830810
2808.407653	190704.056159	55.835815
2807.687289	190579.828717	55.840820
2807.151625	190461.577565	55.845825
2806.587044	190347.657067	55.850829
2806.335471	190210.773409	55.855834
2805.201277	190102.465419	55.860839
2804.726831	189972.958807	55.865844
2804.371418	189849.884134	55.870849
2803.090482	189725.136999	55.875853
2802.940962	189597.857319	55.880858
2801.884796	189485.441674	55.885863
2801.269161	189369.941270	55.890868
2800.697290	189242.665817	55.895873
2799.755834	189118.807992	55.900877
2799.561168	189001.651502	55.905882
2798.389649	188872.271016	55.910887
2798.174324	188759.469493	55.915892
2797.462147	188636.721650	55.920897
2796.396823	188514.437172	55.925901
2795.895394	188387.012934	55.930906
2795.486152	188275.973526	55.935911
2794.593031	188151.016484	55.940916
2793.933375	188034.584887	55.945921
2793.256975	187902.164389	55.950925
2792.787128	187782.688195	55.955930
2792.032148	187672.824532	55.960935
2791.400288	187551.275435	55.965940
2790.483395	187421.018993	55.970945
2789.935849	187313.998526	55.975949
2789.661415	187178.603083	55.980954
2788.775217	187070.797158	55.985959
2788.431716	186936.647398	55.990964
2787.437794	186820.984225	55.995969
2786.886828	186688.458287	56.000973
2786.676410	186565.127592	56.005978
2785.703251	186441.841693	56.010983
2785.089481	186312.990675	56.015988
2784.641146	186189.800445	56.020993
2783.716205	186071.189518	56.025997
2783.280699	185941.102755	56.031002
2782.456042	185825.351689	56.036007
2781.984542	185689.648375	56.041012
2781.102060	185564.391365	56.046017
2780.481354	185437.312227	56.051021
2779.753239	185307.540776	56.056026
2778.963655	185191.951156	56.061031
2778.379593	185061.381588	56.066036
2778.060637	184934.586835	56.071041
2777.084768	184799.843851	56.076045
2776.464362	184670.464262	56.081050
2775.658404	184552.143795	56.086055
2775.182982	184419.294499	56.091060
2774.321416	184299.393351	56.096065
2773.667152	184166.191495	56.101069
2772.959685	184044.676478	56.106074
2772.059014	183926.398114	56.111079
2771.318769	183804.430985	56.116084
2770.956071	183674.390137	56.121089
2770.218424	183562.282074	56.126093
2769.661269	183448.034026	56.131098
2768.917718	183322.952106	56.136103
2768.652719	183199.041398	56.141108
2767.989485	183070.080318	56.146113
2766.990527	182948.512710	56.151117
2766.565155	182814.451815	56.156122
2765.739238	182700.782544	56.161127
2765.100370	182573.778059	56.166132
2764.422631	182450.532704	56.171137
2763.689730	182323.149498	56.176141
2763.070686	182197.453194	56.181146
2762.233386	182085.402845	56.186151
2761.804578	181955.949976	56.191156
2760.848682	181836.884588	56.196161
2760.155487	181716.416828	56.201165
2759.766382	181596.995198	56.206170
2758.965033	181486.899647	56.211175
2758.082412	181355.841350	56.216180
2757.491513	181235.791217	56.221185
2756.898749	181114.813132	56.226189
2756.368614	180994.181635	56.231194
2755.634773	180883.962448	56.236199
2755.165029	180740.133118	56.241204
2754.549961	180631.663873	56.246209
2753.709768	180513.436062	56.251213
2753.384038	180375.716244	56.256218
2752.473201	180257.398568	56.261223
2751.930927	180135.143242	56.266228
2751.322778	180009.324387	56.271233
2750.436622	179887.467677	56.276237
2750.057710	179768.316633	56.281242
2749.060976	179641.097625	56.286247
2748.596402	179515.791724	56.291252
2747.923440	179388.585791	56.296257
2746.995725	179268.963402	56.301261
2746.745889	179147.224269	56.306266
2745.722929	179023.445594	56.311271
2745.067011	178903.018013	56.316276
2744.462588	178775.993864	56.321281
2743.844713	178658.079439	56.326285
2743.418138	178525.978208	56.331290
2742.241783	178418.519329	56.336295
2741.997516	178285.855760	56.341300
2741.039026	178169.077813	56.346305
2740.204052	178043.084516	56.351309
2740.064361	177916.116558	56.356314
2738.904947	177805.591212	56.361319
2738.538906	177671.384406	56.366324
2737.702381	177553.405975	56.371329
2737.369354	177443.106840	56.376333
2736.719987	177320.342447	56.381338
2735.771601	177197.714814	56.386343
2735.316111	177071.257344	56.391348
2734.699018	176946.593804	56.396353
2734.003496	176836.150197	56.401357
2733.429135	176706.889050	56.406362
2732.320425	176587.290303	56.411367
2731.918412	176462.517846	56.416372
2731.042607	176342.107070	56.421377
2730.578052	176207.488179	56.426381
2730.073111	176084.577403	56.431386
2729.061976	175976.920637	56.436391
2728.675665	175853.432140	56.441396
2728.139254	175732.486088	56.446401
2727.215908	175602.088147	56.451405
2726.861045	175493.603745	56.456410
2726.099595	175355.333578	56.461415
2725.369659	175242.610384	56.466420
2724.523923	175114.923476	56.471425
2723.818834	174995.888669	56.476429
2723.757049	174876.828624	56.481434
2722.477052	174753.802985	56.486439
2722.120714	174636.926988	56.491444
2721.663445	174493.206296	56.496449
2720.423550	174373.342320	56.501453
2720.219378	174246.408659	56.506458
2719.574543	174132.581319	56.511463
2719.102960	174007.433160	56.516468
2718.576288	173879.941270	56.521473
2717.796907	173753.888801	56.526477
2717.157631	173621.010403	56.531482
2716.215926	173492.250100	56.536487
2715.447636	173373.217393	56.541492
2714.734236	173246.812690	56.546497
2714.112225	173132.272383	56.551501
2713.525648	173001.002873	56.556506
2712.921670	172882.950314	56.561511
2712.225989	172752.271208	56.566516
2711.594953	172630.128580	56.571521
2710.753404	172508.146851	56.576525
2710.377592	172373.234223	56.581530
2709.580880	172264.752245	56.586535
2708.574741	172139.135069	56.591540
2708.209074	172013.289667	56.596545
2707.484413	171895.246461	56.601549
2706.969205	171767.378024	56.606554
2706.325712	171643.485426	56.611559
2705.589037	171517.357014	56.616564
2705.145241	171390.279688	56.621569
2704.277837	171274.346599	56.626573
2703.719185	171131.531638	56.631578
2702.825983	171025.891595	56.636583
2702.403123	170887.150948	56.641588
2702.181503	170762.914542	56.646593
2701.152285	170641.044661	56.651597
2700.571527	170516.090194	56.656602
2699.634908	170387.962393	56.661607
2699.548524	170256.737292	56.666612
2698.815470	170113.915549	56.671617
2697.898498	169996.747877	56.676621
2697.232652	169859.829757	56.681626
2696.278721	169736.679125	56.686631
2695.673676	169622.883985	56.691636
2694.960364	169489.013997	56.696641
2694.269470	169370.032091	56.701645
2694.026874	169245.040894	56.706650
2693.082129	169114.273573	56.711655
2692.589217	168978.399393	56.716660
2691.952479	168859.423212	56.721665
2690.987844	168740.028838	56.726669
2690.498075	168608.173866	56.731674
2689.755689	168489.597067	56.736679
2689.184341	168357.361681	56.741684
2688.950770	168223.725326	56.746689
2688.107858	168105.928625	56.751693
2687.290956	167969.397265	56.756698
2686.660229	167846.366851	56.761703
2686.039841	167706.422824	56.766708
2685.419353	167586.049295	56.771713
2684.700697	167453.484355	56.776717
2684.155998	167322.240214	56.781722
2683.278005	167198.157516	56.786727
2682.711137	167074.839757	56.791732
2682.238971	166945.174925	56.796737
2681.335573	166810.136507	56.801741
2680.791224	166683.395927	56.806746
2679.867459	166543.542440	56.811751
2679.481577	166420.922958	56.816756
2678.627225	166286.120262	56.821761
2677.918419	166169.376504	56.826765
2677.264060	166030.257913	56.831770
2676.434430	165916.255208	56.836775
2675.834457	165784.287730	56.841780
2675.308076	165661.044524	56.846785
2674.330515	165530.129567	56.851789
2673.758265	165410.022435	56.856794
2673.315107	165285.305040	56.861799
2672.480913	165165.736094	56.866804
2671.952837	165033.187723	56.871809
2671.046030	164931.610279	56.876813
2670.549534	164784.409982	56.881818
2669.815861	164660.961371	56.886823
2669.342911	164536.950558	56.891828
2668.738062	164417.436720	56.896833
2667.827295	164292.466182	56.901837
2667.582724	164155.540287	56.906842
2666.715326	164027.486790	56.911847
2666.063295	163904.345669	56.916852
2665.676344	163766.515611	56.921857
2664.697574	163650.699930	56.926861
2664.164885	163515.805571	56.931866
2663.639495	163396.778361	56.936871
2662.847069	163271.004278	56.941876
2662.239752	163127.731585	56.946881
2661.387722	162996.487951	56.951885
2660.917030	162867.231401	56.956890
2660.121170	162743.557573	56.961895
2659.514660	162613.484300	56.966900
2658.808117	162485.347199	56.971905
2657.991690	162371.569611	56.976909
2657.470097	162221.789965	56.981914
2656.926675	162109.470229	56.986919
2656.496216	161965.614717	56.991924
2655.816367	161837.755409	56.996929
2654.942530	161704.561985	57.001933
2654.655776	161575.878497	57.006938
2653.565889	161453.260102	57.011943
2653.013497	161310.736075	57.016948
2652.372712	161187.577033	57.021953
2651.769083	161055.080629	57.026957
2651.163848	160920.639776	57.031962
2650.270053	160799.581784	57.036967
2649.678713	160654.116990	57.041972
2648.954225	160530.096251	57.046977
2648.490908	160397.885200	57.051981
2648.050557	160265.937988	57.056986
2647.228626	160134.318705	57.061991
2646.460089	159989.418684	57.066996
2645.833003	159867.469838	57.072001
2645.024905	159732.442692	57.077005
2644.604296	159599.401508	57.082010
2643.864299	159460.741346	57.087015
2643.264724	159340.951213	57.092020
2642.824233	159201.736100	57.097025
2641.772056	159073.475391	57.102029
2641.283660	158932.984921	57.107034
2640.587676	158799.659867	57.112039
2639.714393	158667.049910	57.117044
2639.295818	158534.088736	57.122049
2638.265450	158400.373240	57.127053
2638.009938	158274.506394	57.132058
2637.203819	158149.083194	57.137063
2636.664910	158010.040992	57.142068
2635.795788	157875.551928	57.147073
2635.070674	157744.472964	57.152077
2634.641484	157609.470297	57.157082
2633.717233	157486.547159	57.162087
2633.275263	157356.518082	57.167092
2633.003932	157217.080733	57.172097
2631.846884	157084.470955	57.177101
2631.282505	156947.127814	57.182106
2630.668380	156817.560269	57.187111
2630.088864	156675.618791	57.192116
2629.458119	156549.334634	57.197121
2628.708298	156430.086873	57.202125
2628.180128	156278.592142	57.207130
2627.060465	156150.124185	57.212135
2626.639085	156015.228254	57.217140
2626.367018	155875.682082	57.222145
2625.586024	155742.356922	57.227149
2624.499248	155605.407032	57.232154
2624.178489	155477.679443	57.237159
2623.468666	155329.802426	57.242164
2622.792413	155205.551625	57.247169
2622.058659	155065.153989	57.252173
2621.729600	154923.726743	57.257178
2620.715668	154785.993232	57.262183
2620.200484	154666.206043	57.267188
2619.550064	154515.361426	57.272193
2618.690690	154394.460294	57.277197
2617.946714	154253.317698	57.282202
2617.383289	154130.908832	57.287207
2616.855724	153984.839262	57.292212
2616.502994	153848.009023	57.297217
2615.736638	153693.856164	57.302221
2615.232484	153542.369914	57.307226
2614.351998	153385.910451	57.312231
2613.501491	153237.238737	57.317236
2613.387176	153080.913532	57.322241
2612.413825	152986.321529	57.327245
2611.859159	152811.255422	57.332250
2610.789431	152703.739999	57.337255
2610.365757	152532.988946	57.342260
2609.766165	152410.363349	57.347265
2609.043734	152251.685272	57.352269
2608.099954	152143.007776	57.357274
2607.965602	151983.259108	57.362279
2607.121359	151878.989929	57.367284
2606.160760	151708.201116	57.372289
2605.591553	151598.398408	57.377293
2604.726540	151440.509450	57.382298
2604.760427	151290.587884	57.387303
2603.846209	151184.107732	57.392308
2602.918765	151033.843968	57.397313
2602.149415	150884.992073	57.402317
2602.032500	150760.796387	57.407322
2601.020382	150626.829321	57.412327
2600.508332	150468.012160	57.417332
2600.100359	150329.858037	57.422337
2599.506262	150215.259644	57.427341
2598.477968	150046.384002	57.432346
2597.665657	149909.477732	57.437351
2597.007367	149812.684355	57.442356
2596.452516	149645.527835	57.447361
2595.888658	149481.385738	57.452365
2595.267616	149388.870803	57.457370
2594.193403	149245.196624	57.462375
2593.285112	149104.826624	57.467380
2593.408696	148944.162353	57.472385
2593.017677	148785.995161	57.477389
2592.310308	148644.082951	57.482394
2591.426670	148522.076225	57.487399
2590.548238	148412.841674	57.492404
2589.922731	148275.823798	57.497409
2589.084732	148115.354173	57.502413
2588.774148	147951.103521	57.507418
2588.449603	147804.254202	57.512423
2586.955262	147687.761363	57.517428
2586.882085	147518.607892	57.522433
2585.903308	147421.923359	57.527437
2584.909793	147261.228513	57.532442
2584.373585	147105.342073	57.537447
2584.126665	147013.600793	57.542452
2583.355604	146847.509841	57.547457
2582.655863	146685.996158	57.552461
2582.500909	146579.436399	57.557466
2581.392494	146421.432766	57.562471
2580.768241	146266.949610	57.567476
2580.245068	146154.540353	57.572481
2579.543722	146007.377841	57.577485
2579.073017	145829.870983	57.582490
2578.340072	145731.221077	57.587495
2577.086898	145559.227898	57.592500
2576.773047	145431.271791	57.597505
2576.256762	145274.666925	57.602509
2575.480315	145146.226148	57.607514
2574.863433	144991.887901	57.612519
2573.995075	144881.965072	57.617524
2573.946163	144696.722447	57.622529
2572.951931	144585.448203	57.627533
2572.373925	144407.890195	57.632538
2571.773118	144289.286055	57.637543
2570.716606	144131.628892	57.642548
2570.468742	143949.395756	57.647553
2569.020093	143870.993361	57.652557
2568.777950	143703.246932	57.657562
2568.418369	143550.145805	57.662567
2567.605801	143420.205776	57.667572
2567.278704	143248.548831	57.672577
2566.019603	143147.652457	57.677581
2565.591885	142992.696995	57.682586
2565.175393	142829.493871	57.687591
2564.296549	142732.439574	57.692596
2563.618191	142564.984497	57.697601
2562.758668	142402.387533	57.702605
2562.296354	142275.471844	57.707610
2561.366899	142136.889957	57.712615
2561.171556	141972.716090	57.717620
2560.584332	141826.114494	57.722625
2559.490677	141725.514268	57.727629
2558.876853	141554.166404	57.732634
2557.942348	141401.383151	57.737639
2557.937865	141240.816949	57.742644
2557.146285	141098.584022	57.747649
2556.478833	140956.586214	57.752653
2555.786864	140809.828253	57.757658
2555.048242	140696.227902	57.762663
2554.381434	140562.033234	57.767668
2553.482026	140398.665585	57.772673
2552.789429	140261.020394	57.777677
2552.668657	140087.734992	57.782682
2551.473101	139985.873459	57.787687
2550.644312	139808.750446	57.792692
2550.403065	139696.650538	57.797697
2549.641951	139551.497862	57.802701
2548.956019	139396.906655	57.807706
2548.523227	139279.146700	57.812711
2547.560840	139094.921456	57.817716
2547.087316	138981.336425	57.822721
2546.104793	138829.514056	57.827725
2546.351814	138665.097563	57.832730
2545.464595	138545.913337	57.837735
2543.905473	138395.759972	57.842740
2543.370437	138251.543384	57.847745
2543.142017	138122.537296	57.852749
2542.601018	137972.974316	57.857754
2542.266666	137809.937870	57.862759
2541.518482	137645.278203	57.867764
2540.631238	137547.454339	57.872769
2540.051142	137402.728155	57.877773
2539.227914	137220.436311	57.882778
2539.139086	137056.336077	57.887783
2537.844933	136942.063157	57.892788
2537.649092	136766.217390	57.897793
2536.740309	136627.263989	57.902797
2535.871954	136507.754723	57.907802
2534.863434	136348.555515	57.912807
2534.526315	136188.501246	57.917812
2534.554224	136028.301081	57.922817
2533.679392	135904.869829	57.927821
2532.811770	135765.520197	57.932826
2531.680459	135610.396972	57.937831
2530.892407	135463.718877	57.942836
2530.430936	135313.839296	57.947841
2529.725363	135173.552175	57.952845
2529.491334	135037.459346	57.957850
2528.923171	134917.273883	57.962855
2528.397719	134762.402181	57.967860
2527.631503	134600.811358	57.972865
2526.656974	134440.880456	57.977869
2526.348501	134258.106408	57.982874
2525.748415	134106.883132	57.987879
2524.609217	133963.190005	57.992884
2524.108292	133800.583512	57.997889
2523.690716	133666.800062	58.002893
2523.035558	133517.735395	58.007898
2522.293875	133369.688727	58.012903
2521.134888	133224.757585	58.017908
2521.185746	133049.187487	58.022913
2520.122905	132914.950910	58.027917
2519.567809	132800.056476	58.032922
2519.263835	132659.908538	58.037927
2518.162057	132492.133252	58.042932
2517.476622	132342.088759	58.047937
2516.921770	132186.194084	58.052941
2517.042197	132016.538531	58.057946
2516.227562	131850.880885	58.062951
2515.217175	131728.543376	58.067956
2514.452705	131563.819407	58.072961
2513.773555	131404.912998	58.077965
2512.954627	131231.409970	58.082970
2512.402012	131129.071218	58.087975
2511.658397	130984.682696	58.092980
2511.109751	130788.162396	58.097985
2510.493623	130682.634558	58.102989
2509.890892	130531.799103	58.107994
2508.950927	130389.769119	58.112999
2508.281576	130219.817717	58.118004
2508.063093	130064.630862	58.123009
2507.011806	129931.829205	58.128013
2506.639689	129749.907211	58.133018
2506.071878	129554.325798	58.138023
2505.233658	129441.407800	58.143028
2504.699930	129299.877828	58.148033
2503.516079	129137.228645	58.153037
2503.478105	128976.202307	58.158042
2502.441644	128820.999623	58.163047
2501.299623	128666.919488	58.168052
2501.088681	128505.961400	58.173057
2500.284796	128335.445930	58.178061
2499.494454	128183.814731	58.183066
2498.989869	128039.441721	58.188071
2498.407600	127938.364036	58.193076
2498.094942	127785.211503	58.198081
2497.012112	127619.050027	58.203085
2496.262612	127463.098313	58.208090
2495.799995	127305.184332	58.213095
2495.783504	127139.758451	58.218100
2495.039838	126972.480358	58.223105
2493.465353	126869.112824	58.228109
2493.356468	126705.494873	58.233114
2492.541032	126545.063178	58.238119
2491.727120	126417.346072	58.243124
2491.143158	126239.481186	58.248129
2490.673828	126068.012458	58.253133
2490.031123	125932.892181	58.258138
2489.112370	125817.741394	58.263143
2488.367141	125657.900675	58.268148
2487.759844	125476.653818	58.273153
2487.374854	125313.100711	58.278157
2486.624328	125200.694267	58.283162
2486.100185	125040.403093	58.288167
2485.556043	124848.521504	58.293172
2485.084635	124737.761687	58.298177
2483.804532	124567.446877	58.303181
2483.684740	124372.237879	58.308186
2482.862137	124274.665924	58.313191
2482.009998	124083.054490	58.318196
2481.717379	123944.637903	58.323201
2480.693459	123800.115790	58.328205
2480.560722	123607.022327	58.333210
2479.798172	123472.263553	58.338215
2479.045473	123319.459982	58.343220
2478.449052	123141.198505	58.348225
2477.174880	123008.897684	58.353229
2477.083199	122824.882370	58.358234
2475.828998	122694.230666	58.363239
2475.228080	122511.555312	58.368244
2475.349272	122343.864170	58.373249
2474.163600	122240.071920	58.378253
2473.274793	122088.490573	58.383258
2472.480072	121911.271889	58.388263
2472.156916	121742.270976	58.393268
2471.765065	121570.450558	58.398273
2470.864326	121445.729386	58.403277
2470.401967	121298.224256	58.408282
2469.299514	121124.056152	58.413287
2468.289665	120974.633493	58.418292
2468.148781	120815.805261	58.423297
2467.002940	120674.900050	58.428301
2466.932556	120486.149073	58.433306
2466.500466	120355.950018	58.438311
2465.370430	120218.003076	58.443316
2465.255866	120018.679905	58.448321
2464.036395	119903.735732	58.453325
2463.463797	119755.145834	58.458330
2463.122028	119582.511602	58.463335
2462.027106	119420.167513	58.468340
2462.372773	119234.298806	58.473345
2461.061303	119133.769967	58.478349
2460.435000	118951.555100	58.483354
2459.837130	118768.772043	58.488359
2459.115560	118656.522171	58.493364
2457.948246	118470.149709	58.498369
2457.813872	118292.736656	58.503373
2457.426416	118182.479879	58.508378
2456.822708	117987.940848	58.513383
2455.560184	117867.724891	58.518388
2454.626501	117677.468080	58.523393
2454.370470	117511.245214	58.528397
2453.759989	117361.373821	58.533402
2453.071546	117233.370236	58.538407
2452.565672	117040.028911	58.543412
2451.665552	116908.347222	58.548417
2450.987163	116745.750847	58.553421
2450.552133	116550.097885	58.558426
2449.840753	116437.500650	58.563431
2449.228108	116304.697461	58.568436
2448.506022	116120.201095	58.573441
2447.648865	115936.597047	58.578445
2447.412886	115801.902431	58.583450
2446.543592	115668.578347	58.588455
2446.015299	115498.628842	58.593460
2445.377776	115286.045540	58.598465
2444.552689	115168.895730	58.603469
2443.766668	114984.436804	58.608474
2443.594493	114833.089102	58.613479
2442.688506	114678.526502	58.618484
2442.364169	114482.719615	58.623489
2441.317344	114365.932375	58.628493
2440.756380	114194.898824	58.633498
2440.568022	114006.829854	58.638503
2439.850941	113874.214656	58.643508
2438.846590	113686.233009	58.648513
2438.539376	113496.377910	58.653517
2437.298494	113353.668548	58.658522
2437.068190	113229.166681	58.663527
2435.828810	113037.330395	58.668532
2435.438835	112837.262886	58.673537
2434.728967	112697.519396	58.678541
2434.184645	112518.199926	58.683546
2433.836818	112394.279336	58.688551
2432.712002	112239.531681	58.693556
2432.032003	112045.183749	58.698561
2431.647928	111868.699372	58.703565
2430.919893	111721.520176	58.708570
2430.191747	111588.265253	58.713575
2429.243824	111415.535200	58.718580
2428.838494	111218.776786	58.723585
2427.865650	111052.576937	58.728589
2427.409998	110933.947917	58.733594
2426.777272	110766.141328	58.738599
2425.799164	110602.318724	58.743604
2425.995090	110410.129324	58.748609
2424.939539	110308.662320	58.753613
2423.848361	110116.203321	58.758618
2423.777130	109922.587877	58.763623
2422.922339	109767.565466	58.768628
2422.040069	109642.937532	58.773633
2421.260563	109471.977572	58.778637
2420.983371	109292.969200	58.783642
2420.490880	109147.087966	58.788647
2419.260758	108983.366922	58.793652
2418.880875	108803.109340	58.798657
2417.956362	108674.419315	58.803661
2417.899134	108485.223088	58.808666
2416.963321	108336.796380	58.813671
2416.149456	108174.207720	58.818676
2415.599962	108004.122646	58.823681
2414.653368	107867.686589	58.828685
2414.151476	107671.105313	58.833690
2413.675317	107539.894692	58.838695
2413.009871	107346.178235	58.843700
2412.559660	107206.278992	58.848705
2411.474826	107031.260418	58.853709
2410.636792	106893.480233	58.858714
2410.453481	106735.369642	58.863719
2409.566654	106539.683458	58.868724
2408.904321	106410.024925	58.873729
2408.186848	106222.074141	58.878733
2407.789678	106075.574574	58.883738
2406.985349	105908.012804	58.888743
2406.168195	105739.895919	58.893748
2405.449855	105589.529291	58.898753
2404.991913	105425.151722	58.903757
2403.936074	105271.294027	58.908762
2403.808036	105083.195327	58.913767
2402.791829	104951.158224	58.918772
2402.516299	104770.971444	58.923777
2401.591390	104625.585896	58.928781
2401.013088	104463.651235	58.933786
2399.973599	104298.821706	58.938791
2399.880639	104106.322311	58.943796
2399.226864	103961.284856	58.948801
2398.346164	103833.305433	58.953805
2397.708160	103633.771894	58.958810
2397.068141	103463.536855	58.963815
2396.154679	103338.363011	58.968820
2395.938799	103133.431532	58.973825
2395.125360	103005.420573	58.978829
2394.260280	102831.330665	58.983834
2393.750992	102640.488861	58.988839
2392.689533	102527.167581	58.993844
2392.649867	102338.283783	58.998849
2391.679108	102207.510909	59.003853
2391.033956	102014.494507	59.008858
2390.575520	101871.583133	59.013863
2390.058338	101697.103964	59.018868
2389.256997	101539.582811	59.023873
2388.688449	101380.465339	59.028877
2388.380298	101199.790957	59.033882
2387.336554	101020.344679	59.038887
2386.729888	100902.753584	59.043892
2386.037070	100698.914979	59.048897
2385.421107	100514.831327	59.053901
2384.690171	100379.381171	59.058906
2384.057938	100209.339912	59.063911
2383.274223	100039.545928	59.068916
2382.699836	99865.584369	59.073921
2381.807009	99694.325963	59.078925
2381.356410	99550.222500	59.083930
2380.919802	99351.188479	59.088935
2380.136659	99219.920676	59.093940
2379.431365	99040.049230	59.098945
2378.748806	98873.216237	59.103949
2378.284806	98694.463624	59.108954
2377.464408	98536.585431	59.113959
2376.597045	98367.413278	59.118964
2376.279810	98198.066365	59.123969
2375.251457	98028.579749	59.128973
2374.711710	97867.794879	59.133978
2374.200533	97680.590509	59.138983
2373.165370	97554.560313	59.143988
2372.791280	97356.434357	59.148993
2372.351094	97219.726379	59.153997
2371.425562	97018.189868	59.159002
2370.938715	96883.476427	59.164007
2370.064391	96694.320951	59.169012
2369.678153	96561.470742	59.174017
2368.641326	96383.676938	59.179021
2368.503166	96181.040033	59.184026
2367.209589	96041.848892	59.189031
2367.015025	95843.473061	59.194036
2366.421332	95710.768562	59.199041
2365.491019	95542.788026	59.204045
2364.895442	95361.729719	59.209050
2363.834137	95191.109047	59.214055
2363.264116	95028.186648	59.219060
2362.694469	94867.199563	59.224065
2362.078273	94681.178199	59.229069
2361.352318	94562.776307	59.234074
2360.692836	94374.893604	59.239079
2360.098894	94218.258949	59.244084
2359.039036	94053.633030	59.249089
2358.842707	93864.209993	59.254093
2358.220721	93706.359506	59.259098
2357.588644	93575.671259	59.264103
2356.574382	93385.094711	59.269108
2356.330434	93187.257550	59.274113
2355.460367	93084.269959	59.279117
2354.802574	92918.244389	59.284122
2354.241016	92725.084337	59.289127
2353.528355	92534.150235	59.294132
2352.863144	92412.484583	59.299137
2352.174126	92249.449210	59.304141
2351.474080	92061.281812	59.309146
2350.927430	91872.419579	59.314151
2349.970521	91756.174417	59.319156
2349.641485	91577.989684	59.324161
2348.904208	91412.533340	59.329165
2347.983387	91275.360960	59.334170
2347.701366	91057.804352	59.339175
2346.798426	90921.658512	59.344180
2346.382968	90765.140487	59.349185
2345.554212	90592.178743	59.354189
2344.798244	90421.983894	59.359194
2344.513723	90225.720463	59.364199
2343.679937	90084.135258	59.369204
2343.443271	89939.026250	59.374209
2342.439624	89739.432151	59.379213
2341.870115	89555.925573	59.384218
2341.453294	89399.005455	59.389223
2340.332673	89266.759206	59.394228
2339.449624	89086.825004	59.399233
2339.101080	88890.792979	59.404237
2338.571751	88750.727801	59.409242
2338.013519	88545.171661	59.414247
2337.076908	88416.445371	59.419252
2336.645991	88220.337382	59.424257
2335.823075	88081.730501	59.429261
2335.123531	87899.837144	59.434266
2334.869193	87699.730960	59.439271
2334.095316	87574.895389	59.444276
2333.468892	87358.419389	59.449281
2332.698656	87203.726658	59.454285
2332.118137	87053.220627	59.459290
2330.866375	86865.027183	59.464295
2330.655053	86677.824161	59.469300
2330.300867	86504.756453	59.474305
2329.375116	86378.405168	59.479309
2328.300967	86185.916949	59.484314
2328.020487	86004.220443	59.489319
2327.470111	85866.155182	59.494324
2326.496847	85667.582886	59.499329
2326.306130	85481.648527	59.504333
2325.370588	85332.092022	59.509338
2324.943791	85127.948680	59.514343
2323.891405	85001.834825	59.519348
2323.365561	84798.534393	59.524353
2322.607982	84636.010996	59.529357
2322.087590	84455.056680	59.534362
2321.296329	84299.247426	59.539367
2320.800019	84142.384734	59.544372
2320.301074	83938.315005	59.549377
2319.493088	83801.622426	59.554381
2318.624178	83608.015843	59.559386
2317.895958	83444.768054	59.564391
2316.959031	83277.434781	59.569396
2316.893875	83083.616839	59.574401
2315.975427	82948.240307	59.579405
2315.564601	82750.556952	59.584410
2315.038867	82570.259820	59.589415
2314.194131	82451.220545	59.594420
2313.731493	82266.492118	59.599425
2312.631687	82073.772910	59.604429
2312.467125	81892.594088	59.609434
2311.518480	81729.350252	59.614439
2310.743599	81544.468579	59.619444
2310.151719	81397.623442	59.624449
2309.228253	81195.010335	59.629453
2308.518920	81048.820045	59.634458
2308.101841	80865.655843	59.639463
2307.396349	80704.916489	59.644468
2306.807404	80562.392590	59.649473
2305.963440	80376.721076	59.654477
2305.472016	80180.101534	59.659482
2304.973785	80025.640183	59.664487
2304.174780	79841.170422	59.669492
2303.715379	79682.827125	59.674497
2302.907601	79493.558319	59.679501
2302.166943	79349.317812	59.684506
2301.420103	79153.268189	59.689511
2300.691079	78997.659787	59.694516
2300.303065	78816.708051	59.699521
2299.456965	78643.713540	59.704525
2298.871191	78499.574836	59.709530
2297.945881	78305.519668	59.714535
2297.277516	78161.047925	59.719540
2296.935113	77960.953464	59.724545
2296.293767	77814.883058	59.729549
2295.703874	77622.073842	59.734554
2295.073412	77460.771318	59.739559
2294.442466	77299.584201	59.744564
2293.870999	77108.215283	59.749569
2293.319136	76939.585956	59.754573
2292.366161	76763.798335	59.759578
2291.857680	76556.919874	59.764583
2291.135077	76421.643827	59.769588
2290.449606	76225.745627	59.774593
2289.933760	76038.781525	59.779597
2289.063619	75901.086655	59.784602
2288.495858	75693.535788	59.789607
2287.681885	75544.417166	59.794612
2287.141738	75383.680721	59.799617
2285.862643	75199.582483	59.804621
2285.310686	75011.809966	59.809626
2285.513717	74826.840193	59.814631
2284.122785	74706.101500	59.819636
2283.770063	74512.980153	59.824641
2282.671868	74345.111669	59.829645
2282.796014	74159.812090	59.834650
2281.616071	74005.333469	59.839655
2281.149670	73798.451285	59.844660
2280.821376	73633.254202	59.849665
2279.888902	73499.602211	59.854669
2279.172883	73318.890959	59.859674
2278.470231	73124.799524	59.864679
2277.313092	72937.085399	59.869684
2277.213317	72755.242584	59.874689
2276.141972	72605.464456	59.879693
2275.597426	72427.141367	59.884698
2275.157027	72282.650246	59.889703
2274.572658	72085.401787	59.894708
2273.686180	71932.070966	59.899713
2273.217703	71726.521907	59.904718
2272.264474	71603.813203	59.909722
2272.205625	71384.317300	59.914727
2271.117313	71237.225374	59.919732
2270.773686	71054.119246	59.924737
2270.216480	70870.681294	59.929742
2269.456326	70697.646491	59.934746
2268.389795	70533.821126	59.939751
2268.010223	70345.273488	59.944756
2267.510129	70174.564695	59.949761
2267.066904	70006.945733	59.954766
2265.933132	69835.187580	59.959770
2265.359318	69636.384754	59.964775
2264.387830	69482.149051	59.969780
2263.858473	69299.633429	59.974785
2263.540156	69131.894464	59.979790
2262.755944	68954.191836	59.984794
2262.350094	68771.167526	59.989799
2261.026691	68615.936746	59.994804
2260.823463	68418.005912	59.999809
2259.928440	68264.059050	60.004814
2259.493515	68072.058651	60.009818
2258.719099	67901.400542	60.014823
2258.278608	67707.232271	60.019828
2257.568996	67542.001050	60.024833
2256.907164	67378.023971	60.029838
2256.365751	67191.369083	60.034842
2255.749516	67005.747490	60.039847
2254.734650	66823.129434	60.044852
2253.986075	66663.921952	60.049857
2253.240097	66464.589864	60.054862
2252.449992	66297.178181	60.059866
2252.267596	66143.853935	60.064871
2250.932731	65959.363296	60.069876
2250.391073	65783.110968	60.074881
2250.442336	65591.539366	60.079886
2249.706225	65402.884049	60.084890
2249.136567	65272.811768	60.089895
2248.379143	65065.289021	60.094900
2247.943682	64914.744009	60.099905
2247.195485	64705.111838	60.104910
2246.453333	64539.997015	60.109914
2245.800975	64373.004532	60.114919
2244.285931	64180.191542	60.119924
2244.068710	63977.945612	60.124929
2243.157869	63846.924005	60.129934
2242.787211	63645.652580	60.134938
2242.179158	63493.936732	60.139943
2241.527956	63309.632338	60.144948
2240.897029	63117.079310	60.149953
2240.343443	62966.470270	60.154958
2239.889411	62767.988348	60.159962
2238.972113	62613.105746	60.164967
2238.824200	62412.575025	60.169972
2237.930295	62251.591185	60.174977
2237.154001	62064.048503	60.179982
2236.716930	61861.730191	60.184986
2235.885704	61718.120677	60.189991
2234.830454	61512.108511	60.194996
2234.684482	61299.914401	60.200001
2233.886546	61136.465183	60.205006
2232.957459	61000.768461	60.210010
2232.220133	60795.419639	60.215015
2232.042296	60603.437661	60.220020
2231.028843	60463.313857	60.225025
2229.874921	60266.485538	60.230030
2229.856768	60053.446397	60.235034
2228.821536	59927.007757	60.240039
2227.925432	59736.408407	60.245044
2227.736326	59544.670141	60.250049
2227.023067	59375.291069	60.255054
2226.296134	59215.405141	60.260058
2225.549098	59012.986301	60.265063
2224.798168	58875.124403	60.270068
2223.957455	58691.120069	60.275073
2223.813960	58496.425924	60.280078
2222.883801	58366.847732	60.285082
2221.969057	58159.644321	60.290087
2221.752733	57980.469694	60.295092
2221.303951	57780.406594	60.300097
2220.572720	57607.128210	60.305102
2219.596462	57468.201604	60.310106
2219.068488	57268.352831	60.315111
2218.367484	57089.228896	60.320116
2217.854912	56947.783034	60.325121
2217.139240	56747.846240	60.330126
2216.570957	56570.412142	60.335130
2215.960403	56402.126331	60.340135
2215.200143	56202.389257	60.345140
2215.205631	56002.846204	60.350145
2214.106952	55860.444655	60.355150
2213.005505	55656.748490	60.360154
2212.672481	55448.552885	60.365159
2211.686576	55308.751709	60.370164
2211.085115	55137.963374	60.375169
2210.239145	54937.756845	60.380174
2209.848052	54791.982432	60.385178
2208.969037	54605.053539	60.390183
2208.622805	54404.416011	60.395188
2208.025707	54260.732236	60.400193
2207.254500	54055.210503	60.405198
2206.306506	53897.342431	60.410202
2205.960696	53701.073054	60.415207
2205.292767	53552.441313	60.420212
2204.830323	53333.272363	60.425217
2204.012612	53195.128303	60.430222
2203.211766	52984.652405	60.435226
2202.913712	52806.496932	60.440231
2201.810751	52669.519078	60.445236
2201.224543	52454.496930	60.450241
2200.945163	52250.553489	60.455246
2200.010826	52120.108984	60.460250
2199.086872	51922.792563	60.465255
2198.923575	51715.767680	60.470260
2198.394572	51534.491111	60.475265
2197.393502	51360.470132	60.480270
2196.802818	51174.726896	60.485274
2196.523607	50983.649411	60.490279
2195.393435	50799.419359	60.495284
2194.740981	50615.589992	60.500289
2194.473207	50470.817956	60.505294
2193.447952	50314.784196	60.510298
2192.697817	50104.944549	60.515303
2191.477445	49932.063712	60.520308
2191.300649	49743.023781	60.525313
2190.223568	49578.231988	60.530318
2189.627476	49412.596680	60.535322
2189.585566	49222.534864	60.540327
2188.614487	49054.342977	60.545332
2187.754337	48888.368491	60.550337
2187.478684	48685.085108	60.555342
2187.211099	48500.764134	60.560346
2186.210810	48303.885724	60.565351
2185.480231	48163.046179	60.570356
2184.723227	48007.986563	60.575361
2183.911442	47806.825975	60.580366
2183.725708	47603.913999	60.585370
2183.195736	47456.038546	60.590375
2182.237243	47245.161795	60.595380
2181.546554	47098.807847	60.600385
2181.001967	46891.387087	60.605390
2180.321618	46720.647126	60.610394
2179.679630	46552.913954	60.615399
2178.545229	46363.502141	60.620404
2178.054702	46157.770507	60.625409
2177.708451	46026.575263	60.630414
2176.550888	45820.523235	60.635418
2176.579351	45644.854700	60.640423
2175.317209	45463.807064	60.645428
2174.875201	45265.665881	60.650433
2174.341176	45132.106554	60.655438
2173.364447	44932.140490	60.660442
2172.800490	44743.534970	60.665447
2171.829498	44568.576622	60.670452
2172.195530	44363.533544	60.675457
2170.816317	44185.319862	60.680462
2170.015348	44064.600683	60.685466
2169.657560	43875.469011	60.690471
2168.857481	43696.039449	60.695476
2168.240712	43526.996757	60.700481
2167.142461	43342.858595	60.705486
2166.602530	43147.837298	60.710490
2166.642742	42943.153613	60.715495
2165.651621	42786.305303	60.720500
2164.742271	42612.836890	60.725505
2163.845168	42434.542613	60.730510
2163.472219	42237.237735	60.735514
2163.307812	42044.499905	60.740519
2162.541094	41916.868179	60.745524
2161.580785	41714.637724	60.750529
2161.185865	41500.749741	60.755534
2160.538075	41320.160212	60.760538
2160.001799	41143.352525	60.765543
2158.944070	41020.168889	60.770548
2158.419670	40843.463595	60.775553
2157.710637	40664.025851	60.780558
2157.084131	40484.271769	60.785562
2156.646937	40281.459832	60.790567
2155.739006	40082.261522	60.795572
2154.737621	39899.956614	60.800577
2154.739454	39704.175450	60.805582
2153.705597	39565.474123	60.810586
2153.195429	39368.494359	60.815591
2152.009725	39191.131703	60.820596
2151.406051	39010.507415	60.825601
2151.358798	38809.290455	60.830606
2150.389215	38671.147418	60.835610
2149.558166	38488.354796	60.840615
2149.235357	38273.782858	60.845620
2148.806046	38121.437640	60.850625
2147.603503	37950.955818	60.855630
2147.395882	37735.833393	60.860634
2146.923148	37580.080855	60.865639
2145.578671	37403.329575	60.870644
2145.369130	37194.865852	60.875649
2144.785301	37000.446456	60.880654
2143.776958	36871.235956	60.885658
2142.948292	36660.596209	60.890663
2142.514764	36483.506169	60.895668
2141.889242	36326.095062	60.900673
2141.371634	36108.060028	60.905678
2140.406906	35964.564484	60.910682
2140.083931	35760.272823	60.915687
2139.311228	35569.007269	60.920692
2138.285126	35428.124416	60.925697
2138.006362	35227.312493	60.930702
2136.673926	35043.078470	60.935706
2136.482729	34850.502443	60.940711
2135.907860	34719.272121	60.945716
2135.052477	34530.503362	60.950721
2134.262251	34324.071837	60.955726
2133.726052	34195.990803	60.960730
2133.033717	33985.273021	60.965735
2132.690697	33802.667329	60.970740
2131.716320	33645.226202	60.975745
2131.286158	33424.459404	60.980750
2130.636561	33279.312420	60.985754
2130.101660	33076.974122	60.990759
2128.970829	32920.960075	60.995764
2128.403882	32745.370488	61.000769
2128.013687	32555.716010	61.005774
2127.208625	32389.300094	61.010778
2126.686570	32193.087553	61.015783
2125.657429	32024.566549	61.020788
2124.975742	31865.128614	61.025793
2124.459720	31656.051125	61.030798
2123.805085	31519.848178	61.035802
2123.014802	31324.230518	61.040807
2122.251759	31133.480691	61.045812
2121.909752	30942.544616	61.050817
2121.264632	30810.651725	61.055822
2120.507747	30634.280500	61.060826
2120.406201	30433.105150	61.065831
2119.231087	30278.257635	61.070836
2118.699463	30064.191113	61.075841
2118.139468	29903.714868	61.080846
2117.218326	29729.393914	61.085850
2116.957875	29535.852795	61.090855
2115.993015	29384.151324	61.095860
2115.237943	29184.520106	61.100865
2114.756994	29001.548761	61.105870
2113.767899	28847.325166	61.110874
2113.762947	28629.474899	61.115879
2112.837998	28454.122336	61.120884
2111.901176	28267.474744	61.125889
2111.207300	28120.405669	61.130894
2110.407382	27958.855523	61.135898
2109.997296	27745.223576	61.140903
2109.421409	27571.496562	61.145908
2108.560720	27430.982969	61.150913
2107.809864	27254.342507	61.155918
2106.626231	27065.850691	61.160922
2106.797753	26859.254684	61.165927
2105.707366	26709.014333	61.170932
2105.283591	26569.137919	61.175937
2104.410119	26359.531125	61.180942
2103.593363	26219.829089	61.185946
2102.721016	26007.291788	61.190951
2101.940591	25885.486020	61.195956
2101.408204	25696.405389	61.200961
2101.201047	25528.151390	61.205966
2100.108298	25380.326315	61.210970
2099.686921	25165.796837	61.215975
2099.137244	25030.356666	61.220980
2098.197769	24866.605735	61.225985
2097.897484	24676.790326	61.230990
2096.807863	24527.390805	61.235994
2096.135562	24344.664522	61.240999
2095.218524	24180.613021	61.246004
2094.731322	24025.339611	61.251009
2094.144652	23873.066942	61.256014
2093.404116	23698.394769	61.261018
2092.770485	23538.132498	61.266023
2091.912369	23363.999886	61.271028
2091.248181	23210.163369	61.276033
2090.724272	23060.675213	61.281038
2089.968999	22906.498378	61.286042
2089.611183	22718.511852	61.291047
2088.399913	22590.263022	61.296052
2088.063871	22393.599696	61.301057
2087.489272	22238.675031	61.306062
2086.457546	22103.914233	61.311066
2085.957935	21931.360729	61.316071
2085.006846	21785.375268	61.321076
2084.275862	21623.746276	61.326081
2083.469922	21465.387807	61.331086
2082.825910	21315.335903	61.336090
2082.060949	21179.657939	61.341095
2081.560844	21025.333416	61.346100
2080.896506	20869.950057	61.351105
2080.149799	20735.302190	61.356110
2079.572472	20573.358384	61.361114
2078.716010	20411.209074	61.366119
2077.525925	20288.422090	61.371124
2077.292844	20152.061462	61.376129
2076.467803	20009.010615	61.381134
2075.372498	19876.633647	61.386138
2074.757416	19748.875079	61.391143
2073.538324	19605.289647	61.396148
2072.424874	19484.864838	61.401153
2071.844966	19366.151539	61.406158
2070.952824	19258.150323	61.411162
2070.195650	19130.735922	61.416167
2069.132271	19044.163452	61.421172
2068.290951	18930.226898	61.426177
2067.224929	18843.323608	61.431182
2066.289835	18748.732263	61.436186
2065.973903	18661.300462	61.441191
2064.914210	18559.852535	61.446196
2063.791981	18480.264729	61.451201
2063.203738	18405.400534	61.456206
2062.373695	18330.518626	61.461210
2061.821943	18230.906569	61.466215
2060.955349	18146.616093	61.471220
2059.565678	18110.279052	61.476225
2059.124143	18032.488380	61.481230
2058.295656	17973.981226	61.486234
2057.843778	17934.922760	61.491239
2057.181414	17837.197691	61.496244
2056.582986	17817.689850	61.501249
2056.000188	17715.311334	61.506254
2055.064834	17642.425671	61.511258
2054.812706	17596.068175	61.516263
2054.231621	17582.075215	61.521268
2053.610320	17510.638570	61.526273
2052.477896	17426.086734	61.531278
2052.335334	17352.046119	61.536282
2051.680752	17331.049002	61.541287
2050.714825	17253.442934	61.546292
2050.302761	17168.430880	61.551297
2049.729457	17135.826530	61.556302
2048.788759	17063.630783	61.561306
2048.594968	16973.763038	61.566311
2047.817812	16957.830967	61.571316
2047.207436	16874.250515	61.576321
2047.105628	16815.107125	61.581326
2045.687871	16766.718655	61.586330
2045.483423	16656.871320	61.591335
2044.737032	16622.390087	61.596340
2044.335711	16537.330462	61.601345
2043.452738	16507.321154	61.606350
2042.653956	16406.452517	61.611354
2042.577138	16370.507186	61.616359
2041.486484	16298.823845	61.621364
2040.946585	16215.663577	61.626369
2040.335406	16177.585153	61.631374
2039.645092	16094.316609	61.636378
2038.908492	16030.722903	61.641383
2038.348829	15962.574401	61.646388
2037.412252	15919.773040	61.651393
2037.100311	15845.106080	61.656398
2036.667575	15784.635830	61.661402
2035.773022	15716.804094	61.666407
2034.894307	15658.626142	61.671412
2034.215693	15566.398938	61.676417
2033.845168	15536.277356	61.681422
2032.676237	15470.551032	61.686426
2032.124576	15366.647227	61.691431
2031.846064	15347.879634	61.696436
2031.352526	15246.869621	61.701441
2030.717463	15233.211460	61.706446
2029.336403	15150.048666	61.711450
2029.342120	15053.853550	61.716455
2028.023571	15044.817220	61.721460
2027.400795	14958.370461	61.726465
2027.360666	14881.181407	61.731470
2026.541256	14808.611280	61.736474
2025.951174	14766.702076	61.741479
2025.310068	14729.847012	61.746484
2024.462026	14625.303400	61.751489
2024.282324	14549.041751	61.756494
2023.790269	14489.438075	61.761498
2023.061361	14404.986389	61.766503
2022.305583	14351.284504	61.771508
2021.586944	14329.150607	61.776513
2020.883473	14244.174007	61.781518
2019.490292	14173.930403	61.786522
2019.417704	14085.508165	61.791527
2019.143525	14014.120952	61.796532
2018.138287	13988.979652	61.801537
2017.223944	13940.740908	61.806542
2016.602752	13883.121614	61.811546
2015.952408	13799.290675	61.816551
2015.261318	13725.501702	61.821556
2014.514243	13656.814922	61.826561
2014.568764	13561.430327	61.831566
2013.433856	13490.509759	61.836570
2013.180259	13483.260823	61.841575
2012.126835	13400.394210	61.846580
2011.624367	13320.513189	61.851585
2011.139206	13239.951563	61.856590
2010.152865	13188.761689	61.861594
2009.755346	13155.424718	61.866599
2008.657048	13071.452939	61.871604
2008.357932	12974.359271	61.876609
2007.414853	12939.868830	61.881614
2006.418320	12909.145201	61.886618
2006.000559	12816.806568	61.891623
2005.371402	12737.082864	61.896628
2004.586768	12719.164671	61.901633
2003.802021	12631.667497	61.906638
2003.483496	12562.132865	61.911642
2002.618545	12539.488793	61.916647
2002.175855	12463.766152	61.921652
2001.626257	12396.812845	61.926657
2000.959087	12361.016771	61.931662
1999.656964	12286.412466	61.936666
1999.901780	12198.539361	61.941671
1998.970548	12182.936019	61.946676
1998.553110	12085.164903	61.951681
1997.976541	12028.584786	61.956686
1996.806039	12003.720987	61.961690
1996.336116	11895.178131	61.966695
1995.682509	11853.821237	61.971700
1995.172863	11783.052257	61.976705
1994.704240	11714.277789	61.981710
1993.391572	11647.649910	61.986714
1992.829076	11604.035522	61.991719
1992.024617	11511.640341	61.996724
1991.741936	11489.980533	62.001729
1990.627746	11419.735093	62.006734
1990.119140	11351.158586	62.011738
1989.854941	11313.333534	62.016743
1989.137722	11227.662769	62.021748
1988.556494	11201.248225	62.026753
1987.640982	11113.995188	62.031758
1987.303024	11034.113700	62.036762
1986.465621	11002.899816	62.041767
1985.522149	10933.123877	62.046772
1985.337297	10841.724698	62.051777
1984.537907	10825.170401	62.056782
1983.734433	10763.125605	62.061786
1983.112970	10661.951980	62.066791
1982.492321	10598.783294	62.071796
1981.694953	10583.551726	62.076801
1980.707932	10490.762937	62.081806
1980.588121	10415.410964	62.086810
1979.843285	10398.443723	62.091815
1979.002116	10309.489552	62.096820
1978.505392	10254.117680	62.101825
1978.039096	10209.314481	62.106830
1977.100224	10120.208091	62.111834
1976.426303	10073.661052	62.116839
1975.990501	9991.383161	62.121844
1975.133847	9964.537564	62.126849
1974.769324	9868.918809	62.131854
1973.696738	9841.719133	62.136858
1973.271634	9742.002216	62.141863
1972.263876	9722.452178	62.146868
1971.954830	9631.213187	62.151873
1971.299503	9593.894770	62.156878
1970.617155	9520.309551	62.161882
1970.095032	9485.416426	62.166887
1969.179221	9395.083852	62.171892
1968.594140	9354.715448	62.176897
1968.141192	9256.119776	62.181902
1967.148110	9232.450162	62.186906
1966.966341	9145.770969	62.191911
1965.827735	9096.034515	62.196916
1965.435349	9022.752058	62.201921
1964.529612	8969.510529	62.206926
1964.257321	8892.349420	62.211930
1963.261914	8863.531058	62.216935
1962.447574	8780.793669	62.221940
1961.983991	8720.138414	62.226945
1961.185157	8682.409566	62.231950
1960.466002	8588.715905	62.236954
1959.910876	8561.550040	62.241959
1959.063069	8507.761350	62.246964
1958.708655	8443.599776	62.251969
1957.905431	8373.950747	62.256974
1956.897688	8341.480394	62.261978
1956.921612	8268.177365	62.266983
1956.109035	8190.302539	62.271988
1955.100750	8153.694178	62.276993
1954.767783	8075.111142	62.281998
1953.948240	8038.941702	62.287002
1953.420987	7966.473127	62.292007
1952.609353	7897.787717	62.297012
1951.789558	7855.795310	62.302017
1951.149004	7786.286501	62.307022
1950.476045	7750.316958	62.312026
1950.182223	7693.378539	62.317031
1949.267819	7619.189486	62.322036
1948.676190	7589.502506	62.327041
1948.112759	7510.871064	62.332046
1947.524450	7438.808382	62.337050
1946.625929	7405.330371	62.342055
1945.807799	7319.159953	62.347060
1945.538550	7300.959982	62.352065
1945.210739	7202.154866	62.357070
1944.221003	7171.186948	62.362074
1943.516838	7071.117199	62.367079
1942.946780	7043.028422	62.372084
1941.885707	7003.133984	62.377089
1940.950814	6920.234370	62.382094
1940.750077	6853.028149	62.387098
1939.719382	6823.783926	62.392103
1939.528612	6747.704007	62.397108
1938.995250	6688.320332	62.402113
1938.370885	6665.973948	62.407118
1937.263466	6596.129894	62.412122
1937.194339	6503.831482	62.417127
1936.600496	6476.337575	62.422132
1935.434165	6410.494272	62.427137
1935.242526	6314.577777	62.432142
1934.434540	6275.400789	62.437146
1933.503097	6240.272612	62.442151
1933.097771	6136.956893	62.447156
1932.246243	6111.483615	62.452161
1931.552740	6025.866476	62.457166
1930.658439	5978.689256	62.462170
1930.086690	5936.440481	62.467175
1929.542500	5853.061251	62.472180
1928.684097	5795.710967	62.477185
1928.152519	5777.890519	62.482190
1927.260311	5715.128713	62.487194
1927.039853	5625.551812	62.492199
1926.121898	5556.370385	62.497204
1925.375689	5514.559870	62.502209
1924.754118	5491.190242	62.507214
1924.249165	5412.511341	62.512218
1923.883900	5351.252805	62.517223
1923.342092	5293.563174	62.522228
1922.234117	5242.187515	62.527233
1921.861605	5163.908519	62.532238
1920.944248	5122.510393	62.537242
1920.297440	5073.298944	62.542247
1919.379695	4995.160236	62.547252
1918.544785	4973.896469	62.552257
1918.632719	4894.496030	62.557262
1917.574366	4840.197239	62.562266
1916.902168	4790.891387	62.567271
1916.375277	4711.890812	62.572276
1915.335449	4693.661784	62.577281
1915.057736	4611.202383	62.582286
1914.073370	4564.973863	62.587290
1913.582372	4497.583856	62.592295
1912.850081	4460.312258	62.597300
1912.293718	4407.943384	62.602305
1911.701932	4340.783040	62.607310
1910.802557	4289.676510	62.612314
1910.226978	4233.448352	62.617319
1909.666937	4180.444409	62.622324
1908.842767	4126.819313	62.627329
1908.287027	4071.042902	62.632334
1907.285022	4016.763451	62.637338
1906.990901	3967.909033	62.642343
1906.115984	3912.157078	62.647348
1905.271224	3856.777526	62.652353
1905.142761	3802.148053	62.657358
1904.238381	3741.888743	62.662362
1903.897409	3700.550612	62.667367
1903.124603	3650.687268	62.672372
1902.866013	3582.242480	62.677377
1901.855648	3509.575893	62.682382
1900.924729	3476.492877	62.687386
1900.177137	3402.144746	62.692391
1899.461042	3361.609222	62.697396
1898.957830	3310.945577	62.702401
1898.521681	3233.356497	62.707406
1897.661687	3210.470775	62.712410
1897.222303	3153.971198	62.717415
1896.593795	3098.994713	62.722420
1895.648135	3039.139158	62.727425
1895.475127	2996.011434	62.732430
1894.544286	2938.608885	62.737434
1894.029284	2859.786725	62.742439
1893.020782	2807.428311	62.747444
1892.286342	2779.189241	62.752449
1891.872824	2689.751540	62.757454
1891.222258	2655.168561	62.762458
1890.532839	2594.826229	62.767463
1889.938964	2532.232550	62.772468
1889.202782	2493.592077	62.777473
1888.576772	2414.355430	62.782478
1887.345868	2358.639101	62.787482
1887.019810	2334.600687	62.792487
1886.496980	2280.134121	62.797492
1885.558480	2215.765443	62.802497
1884.956427	2173.065479	62.807502
1884.313410	2105.317899	62.812506
1883.495168	2086.516020	62.817511
1883.060997	2006.637633	62.822516
1882.295891	1970.808828	62.827521
1881.942462	1909.854541	62.832526
1880.965290	1856.215543	62.837530
1880.535862	1818.945187	62.842535
1879.995891	1753.155833	62.847540
1878.996974	1704.484732	62.852545
1878.254815	1651.347755	62.857550
1877.376018	1612.970401	62.862554
1877.100510	1542.246360	62.867559
1876.410422	1501.699265	62.872564
1875.505833	1464.463459	62.877569
1875.060522	1414.574695	62.882574
1874.049875	1366.310316	62.887578
1873.486647	1326.467436	62.892583
1872.949091	1270.752448	62.897588
1872.323930	1224.576844	62.902593
1871.887124	1174.263333	62.907598
1871.077867	1135.740579	62.912602
1870.588239	1066.535242	62.917607
1870.081632	1006.257210	62.922612
1869.288529	993.054294	62.927617
1868.684908	896.846686	62.932622
1867.680220	880.693790	62.937626
1866.930318	811.389060	62.942631
1866.201160	760.435831	62.947636
1865.117286	749.807201	62.952641
1864.864953	671.389637	62.957646
1864.018462	660.728119	62.962650
1863.465602	582.844451	62.967655
1862.814250	575.176629	62.972660
1862.061334	517.946994	62.977665
1861.712783	463.379932	62.982670
1860.800040	440.517216	62.987674
1859.992728	391.686069	62.992679
1859.602894	342.438730	62.997684
1858.644806	312.398903	63.002689
1858.222839	262.072010	63.007694
1857.250289	224.717726	63.012698
1856.916610	174.389736	63.017703
1856.123138	136.355985	63.022708
1855.436464	102.626108	63.027713
1854.587281	73.113525	63.032718
1853.549212	28.686694	63.037722
1852.907650	-1.830068	63.042727
1852.233665	-32.363694	63.047732
1851.238779	-66.291815	63.052737
1850.316486	-88.885676	63.057742
1848.299376	-78.867536	63.062746
1842.165553	61.527640	63.067751
1842.786659	60.112347	63.072756
1844.286903	59.823730	63.077761
1846.045148	45.019759	63.082766
1846.105188	45.801863	63.087770
1845.927872	44.149068	63.092775
1844.563620	51.103801	63.097780
1843.142160	55.177155	63.102785
1842.264380	58.533432	63.107790
1841.662832	63.271375	63.112794
1841.381576	57.992433	63.117799
1841.049851	57.021721	63.122804
1840.226799	62.701551	63.127809
1839.150722	50.520542	63.132814
1838.462074	71.542810	63.137818
1837.792111	67.369490	63.142823
1836.924571	47.795964	63.147828
1836.063740	79.650521	63.152833
1836.495022	57.264146	63.157838
1836.167340	70.713582	63.162842
1835.076995	73.356159	63.167847
1834.609682	63.856997	63.172852
1833.100664	66.383126	63.177857
1832.730351	54.861170	63.182862
1832.258463	79.676179	63.187866
1831.582332	63.744859	63.192871
1830.982032	62.305873	63.197876
1829.876283	76.528533	63.202881
1829.827235	55.976672	63.207886
1828.795960	71.204606	63.212890
1828.475212	67.332224	63.217895
1827.548267	53.881787	63.222900
1826.393353	74.216445	63.227905
1826.005073	66.929748	63.232910
1825.697770	67.576218	63.237914
1825.402750	62.051888	63.242919
1824.431353	60.624516	63.247924
1823.432964	69.005044	63.252929
1823.384183	77.906565	63.257934
1822.409584	60.825770	63.262938
1821.904837	76.387991	63.267943
1820.925268	69.341828	63.272948
1820.387613	70.707672	63.277953
1820.404860	66.647590	63.282958
1819.002384	67.203026	63.287962
1818.132434	67.008457	63.292967
1817.733959	69.605843	63.297972
1817.028742	69.861344	63.302977
1816.866781	69.879206	63.307982
1815.724171	79.788585	63.312986
1815.071529	67.571882	63.317991
1814.544999	62.066967	63.322996
1813.897377	49.717023	63.328001
1813.513550	65.591183	63.333006
1812.261472	74.716872	63.338010
1811.723710	72.563084	63.343015
1811.427123	65.105719	63.348020
1810.505538	62.984490	63.353025
1810.014287	74.332657	63.358030
1809.259367	67.857939	63.363034
1808.417325	70.248220	63.368039
1807.834301	58.331124	63.373044
1806.979421	65.260193	63.378049
1807.123601	75.356328	63.383054
1806.136600	59.203156	63.388058
1805.500683	75.200929	63.393063
1805.333012	71.450897	63.398068
1804.477783	73.333932	63.403073
1803.990920	71.222525	63.408078
1803.018627	65.778928	63.413082
1801.509965	64.545679	63.418087
1801.182909	59.130517	63.423092
1800.985860	64.452347	63.428097
1799.750415	71.555386	63.433102
1799.143726	65.076059	63.438106
1799.052505	64.909231	63.443111
1798.251080	52.493828	63.448116
1797.153961	57.137006	63.453121
1796.635003	68.245148	63.458126
1796.001071	45.230020	63.463130
1795.428080	64.830472	63.468135
1795.192732	69.114475	63.473140
1794.214386	69.203623	63.478145
1794.164359	61.973610	63.483150
1793.160136	48.421929	63.488154
1792.604277	88.101551	63.493159
1791.619712	58.462307	63.498164
1790.389012	58.500066	63.503169
1790.153427	74.349119	63.508174
1789.442697	65.133040	63.513178
1789.519516	58.488419	63.518183
1788.277401	77.715758	63.523188
1787.597515	61.578481	63.528193
1787.039207	56.496500	63.533198
1786.580315	55.003534	63.538202
1785.941367	77.590091	63.543207
1785.548149	46.865103	63.548212
1783.869333	61.830017	63.553217
1783.123861	69.858170	63.558222
1783.002592	70.462489	63.563226
1782.431761	58.265931	63.568231
1781.571010	74.323059	63.573236
1780.835849	61.770982	63.578241
1780.064810	66.898538	63.583246
1779.695932	67.720365	63.588250
1779.130974	54.728119	63.593255
1778.478382	68.191298	63.598260
1778.046445	48.285292	63.603265
1777.574191	72.056432	63.608270
1777.054987	58.153352	63.613274
1775.534985	58.355325	63.618279
1774.787697	74.796547	63.623284
1773.830652	67.075069	63.628289
1773.626885	68.331134	63.633294
1773.396446	63.367397	63.638298
1772.860287	71.445891	63.643303
1772.279429	56.472426	63.648308
1771.679314	68.815557	63.653313
1770.977734	67.640242	63.658318
1770.003179	49.182846	63.663322
1769.037959	77.523290	63.668327
1768.647543	54.441108	63.673332
1767.885657	68.807863	63.678337
1767.585920	58.181434	63.683342
1766.817422	59.568175	63.688346
1766.190567	65.208985	63.693351
1765.156678	69.551987	63.698356
1764.387648	50.005432	63.703361
1763.769953	58.569938	63.708366
1763.046423	63.976949	63.713370
1762.625168	59.046670	63.718375
1762.212321	51.948394	63.723380
1761.493572	66.289374	63.728385
1761.138206	60.388298	63.733390
1759.657416	58.638155	63.738394
1758.791073	70.939990	63.743399
1758.558323	53.350363	63.748404
1757.583566	58.954958	63.753409
1757.157838	52.744948	63.758414
1756.665017	71.101117	63.763418
1756.354358	68.356208	63.768423
1755.892722	45.684311	63.773428
1755.222998	78.426272	63.778433
1754.460841	56.629955	63.783438
1753.325946	61.208189	63.788442
1752.422256	76.690265	63.793447
1752.240339	40.535587	63.798452
1751.409066	85.563622	63.803457
1751.096505	45.309226	63.808462
1750.192133	51.277946	63.813466
1749.186285	66.156513	63.818471
1748.681063	70.393491	63.823476
1747.521767	64.143857	63.828481
1747.137053	49.922981	63.833486
1746.534050	64.936264	63.838490
1746.149707	61.969677	63.843495
1746.341899	42.117538	63.848500
1745.153053	75.695687	63.853505
1744.820371	54.761550	63.858510
1743.984373	62.875043	63.863514
1743.191069	72.823583	63.868519
1742.655649	63.792565	63.873524
1741.090986	62.601360	63.878529
1740.350942	48.447954	63.883534
1739.706736	66.257320	63.888538
1739.153815	71.329749	63.893543
1738.893322	56.040502	63.898548
1738.338745	71.087101	63.903553
1737.888548	62.878309	63.908558
1737.636085	58.427416	63.913562
1736.636155	59.499269	63.918567
1735.859665	58.332707	63.923572
1734.661288	64.836966	63.928577
1734.487771	59.507816	63.933582
1734.129879	50.700920	63.938586
1732.621687	54.846448	63.943591
1731.838181	60.614639	63.948596
1731.374844	44.994931	63.953601
1731.239982	55.073854	63.958606
1730.629947	59.710664	63.963610
1729.805623	44.668663	63.968615
1729.670209	63.666631	63.973620
1728.223492	77.922968	63.978625
1727.557449	40.014401	63.983630
1727.015387	76.567947	63.988634
1726.450448	47.090782	63.993639
1726.136589	71.051220	63.998644
1725.284492	40.323459	64.003649
1724.262160	76.716742	64.008654
1723.293348	53.783204	64.013658
1722.708380	72.079893	64.018663
1722.456973	55.504033	64.023668
1721.721551	66.197139	64.028673
1721.450858	50.874830	64.033678
1720.587667	73.050730	64.038682
1720.344240	56.822097	64.043687
1719.197237	45.975442	64.048692
1718.055220	66.123566	64.053697
1718.046593	32.261028	64.058702
1717.209082	76.470031	64.063706
1717.139296	56.957516	64.068711
1715.626261	61.879661	64.073716
1714.539241	67.732329	64.078721
1714.326113	49.739070	64.083726
1713.902509	54.806729	64.088730
1713.345916	60.624039	64.093735
1713.279167	60.752939	64.098740
1712.401022	70.235579	64.103745
1711.386700	59.203850	64.108750
1710.490982	61.145380	64.113754
1709.985727	68.750632	64.118759
1709.580287	61.853031	64.123764
1707.984673	56.532127	64.128769
1707.323615	68.399257	64.133774
1706.784472	64.596273	64.138778
1706.325813	57.554167	64.143783
1706.103034	54.205551	64.148788
1705.629420	46.210224	64.153793
1705.244228	57.128392	64.158798
1704.647323	63.171296	64.163802
1703.078507	63.321140	64.168807
1702.832785	46.266591	64.173812
1702.340562	69.589899	64.178817
1701.387816	57.348374	64.183822
1700.267845	44.311853	64.188826
1699.512620	70.890655	64.193831
1699.213114	58.275732	64.198836
1698.348801	63.711424	64.203841
1698.082229	48.431046	64.208846
1697.666253	56.307532	64.213850
1697.166577	66.715628	64.218855
1696.199804	49.679404	64.223860
1695.365342	55.901957	64.228865
1694.833554	40.403522	64.233870
1694.259940	57.829519	64.238874
1693.728005	55.610182	64.243879
1692.589820	43.541623	64.248884
1691.696208	73.546935	64.253889
1691.437247	50.483335	64.258894
1691.134644	51.288339	64.263898
1690.292473	71.721580	64.268903
1690.018601	58.203754	64.273908
1688.667587	54.215918	64.278913
1687.871967	54.473197	64.283918
1687.559682	63.124823	64.288922
1687.069499	56.094037	64.293927
1686.265872	55.447447	64.298932
1684.995092	59.197339	64.303937
1684.315709	57.980677	64.308942
1684.103040	64.842469	64.313946
1683.453650	65.413981	64.318951
1683.274328	53.442276	64.323956
1682.493803	49.516797	64.328961
1681.946132	46.352246	64.333966
1680.972297	72.489548	64.338970
1680.366696	62.036292	64.343975
1680.015372	49.705569	64.348980
1678.938359	51.996015	64.353985
1678.052034	65.496325	64.358990
1677.597049	56.138752	64.363994
1677.202315	58.018069	64.368999
1676.543662	43.468582	64.374004
1675.241629	64.258695	64.379009
1674.699502	55.222460	64.384014
1674.158824	58.285557	64.389018
1673.085058	56.967541	64.394023
1673.244448	59.335992	64.399028
1672.336931	66.475299	64.404033
1672.258459	59.544698	64.409038
1671.203058	55.897838	64.414042
1670.365588	52.610589	64.419047
1670.244679	57.786289	64.424052
1668.651096	63.113900	64.429057
1668.110404	55.050388	64.434062
1667.273721	55.569653	64.439066
1666.391807	66.224537	64.444071
1666.401644	52.243781	64.449076
1665.853313	73.163347	64.454081
1665.807323	53.057309	64.459086
1665.029645	54.905990	64.464090
1663.919893	62.864293	64.469095
1663.470965	49.369556	64.474100
1662.491297	69.624370	64.479105
1661.660839	48.958564	64.484110
1660.607512	62.792896	64.489114
1660.398177	49.745789	64.494119
1659.780008	50.395923	64.499124
1659.385406	57.121034	64.504129
1658.755589	51.195768	64.509134
1657.630019	55.237986	64.514138
1656.878049	66.040961	64.519143
1656.595685	51.204632	64.524148
1656.178912	53.637789	64.529153
1655.377916	48.652740	64.534158
1654.435321	55.065937	64.539162
1653.404760	70.520869	64.544167
1653.265311	32.987607	64.549172
1652.777682	70.108043	64.554177
1652.162930	55.069050	64.559182
1651.201050	70.233962	64.564186
1650.342384	52.650749	64.569191
1650.227262	58.404253	64.574196
1649.582258	48.217465	64.579201
1648.308433	56.462019	64.584206
1647.782974	54.014591	64.589210
1646.903935	59.876820	64.594215
1647.025979	47.343189	64.599220
1646.054372	54.935787	64.604225
1645.360613	48.451422	64.609230
1644.577160	50.524946	64.614234
1643.688073	62.324224	64.619239
1643.128466	51.384305	64.624244
1642.628665	56.680111	64.629249
1642.218916	54.125997	64.634254
1641.243475	58.259489	64.639258
1640.352323	61.416107	64.644263
1640.253523	39.344204	64.649268
1639.568681	60.392663	64.654273
1638.909597	53.601603	64.659278
1637.940557	44.343049	64.664282
1637.234339	71.085948	64.669287
1636.750850	49.835202	64.674292
1636.099394	37.717750	64.679297
1635.413444	66.687155	64.684302
1634.332700	41.606387	64.689306
1633.787905	54.248226	64.694311
1633.600259	50.641735	64.699316
1632.989672	58.616946	64.704321
1632.178962	51.780590	64.709326
1631.639186	61.799255	64.714330
1630.557642	59.094821	64.719335
1630.355503	60.062063	64.724340
1629.679726	64.963218	64.729345
1628.894683	57.775864	64.734350
1628.036961	50.775096	64.739354
1627.388525	67.684731	64.744359
1627.431180	40.626276	64.749364
1625.882162	68.610030	64.754369
1625.471535	54.416957	64.759374
1624.822263	56.462865	64.764378
1624.296638	68.064072	64.769383
1623.747958	41.309277	64.774388
1622.400181	83.076303	64.779393
1622.065261	46.114950	64.784398
1621.390683	67.893472	64.789402
1621.216775	67.099563	64.794407
1620.742761	58.907204	64.799412
1619.542489	62.934498	64.804417
1618.652448	65.237844	64.809422
1618.497277	55.935161	64.814426
1617.451346	54.081332	64.819431
1616.834635	58.399113	64.824436
1615.820958	65.455954	64.829441
1615.247150	45.771240	64.834446
1614.733549	69.020669	64.839450
1614.315099	53.687166	64.844455
1614.119078	52.251820	64.849460
1613.097570	64.993051	64.854465
1612.218390	58.976526	64.859470
1611.722156	62.139803	64.864474
1611.081477	64.304194	64.869479
1610.069006	59.660247	64.874484
1609.040437	63.890497	64.879489
1608.601529	60.949949	64.884494
1608.433094	56.235000	64.889498
1607.802605	65.962163	64.894503
1607.816805	57.791597	64.899508
1606.791270	60.556425	64.904513
1605.857021	54.197004	64.909518
1605.371602	62.743675	64.914522
1603.779158	69.324779	64.919527
1603.457689	60.496353	64.924532
1602.823943	63.392903	64.929537
1602.580598	51.087623	64.934542
1602.225735	56.841364	64.939546
1601.219510	59.598396	64.944551
1600.402090	70.039632	64.949556
1599.798154	66.913996	64.954561
1599.163489	52.597257	64.959566
1597.861763	49.159866	64.964570
1597.180611	55.610392	64.969575
1596.781355	62.199060	64.974580
1596.337455	53.219784	64.979585
1595.987612	60.705741	64.984590
1595.696438	58.167491	64.989594
1594.497757	66.318136	64.994599
1593.711566	61.173063	64.999604
1593.139263	56.113857	65.004609
1592.760190	50.148779	65.009614
1592.144321	50.871100	65.014618
1590.984173	49.120581	65.019623
1590.256362	49.937954	65.024628
1589.756713	65.844699	65.029633
1589.541629	51.740420	65.034638
1588.690309	47.824642	65.039642
1587.636279	52.371167	65.044647
1587.137014	47.218365	65.049652
1586.600644	56.682999	65.054657
1585.839299	52.458048	65.059662
1585.026643	50.228141	65.064666
1584.136544	55.434576	65.069671
1584.091725	47.889961	65.074676
1583.577922	51.743559	65.079681
1582.877525	63.241648	65.084686
1582.017342	51.084828	65.089690
1581.006496	59.199325	65.094695
1580.769786	48.700125	65.099700
1580.203690	60.397642	65.104705
1578.935902	50.513238	65.109710
1578.292403	52.209744	65.114714
1577.798390	56.536423	65.119719
1577.183818	46.078333	65.124724
1576.590834	66.870945	65.129729
1576.172655	58.756457	65.134734
1575.166164	46.055204	65.139738
1574.079698	53.956219	65.144743
1573.825086	46.383436	65.149748
1573.437585	44.574829	65.154753
1572.752442	52.905654	65.159758
1572.682952	55.428726	65.164762
1571.172983	54.336165	65.169767
1570.807130	49.542204	65.174772
1570.216895	51.307518	65.179777
1569.532049	55.487903	65.184782
1568.613193	54.123245	65.189786
1568.001479	56.161622	65.194791
1567.614054	54.884418	65.199796
1566.266171	69.054148	65.204801
1565.370708	50.905991	65.209806
1565.211359	54.856239	65.214810
1564.263430	59.092615	65.219815
1564.220866	51.244877	65.224820
1563.876133	61.664632	65.229825
1563.241763	53.980298	65.234830
1562.294189	46.523918	65.239834
1561.545349	54.595217	65.244839
1561.274092	43.718326	65.249844
1559.818230	53.959803	65.254849
1559.162786	54.642690	65.259854
1558.791523	61.818250	65.264858
1558.040280	56.177223	65.269863
1557.950514	51.560166	65.274868
1556.724570	51.841699	65.279873
1556.110462	58.205892	65.284878
1555.591994	52.521578	65.289882
1554.741851	58.932732	65.294887
1554.521654	56.384788	65.299892
1553.461537	51.299022	65.304897
1552.506914	49.036491	65.309902
1552.237782	51.108749	65.314906
1551.931714	52.652307	65.319911
1551.280777	52.150228	65.324916
1550.089327	57.369860	65.329921
1549.637693	56.610621	65.334926
1548.942875	54.324159	65.339930
1547.784298	51.978919	65.344935
1547.526716	53.946844	65.349940
1546.422132	54.237484	65.354945
1546.160027	59.337849	65.359950
1546.049674	49.920832	65.364954
1545.117060	51.013598	65.369959
1544.260356	50.080606	65.374964
1543.656278	50.643376	65.379969
1543.036143	50.707243	65.384974
1542.708371	44.196305	65.389978
1541.316788	56.036013	65.394983
1541.024122	45.380140	65.399988
1540.681473	51.485167	65.404993
1539.961101	53.843578	65.409998
1538.796977	55.050398	65.415002
1537.902261	55.282467	65.420007
1537.781691	47.699432	65.425012
1537.339091	56.280302	65.430017
1536.515616	49.766122	65.435022
1535.718993	53.473858	65.440026
1534.836512	53.820675	65.445031
1534.571722	49.986763	65.450036
1533.774558	52.668025	65.455041
1532.940043	48.016342	65.460046
1532.352053	48.485097	65.465050
1531.809179	55.083970	65.470055
1531.533317	47.550840	65.475060
1530.199980	50.137526	65.480065
1529.562576	50.388637	65.485070
1529.071801	46.964357	65.490074
1528.941451	44.280721	65.495079
1527.861139	50.226997	65.500084
1526.594437	53.077478	65.505089
1526.350253	49.079450	65.510094
1525.854017	55.809681	65.515098
1525.355615	50.306685	65.520103
1524.555718	43.553808	65.525108
1523.339917	45.670830	65.530113
1522.994450	49.283232	65.535118
1522.933302	54.719083	65.540122
1521.972531	70.777946	65.545127
1521.177394	43.188758	65.550132
1520.349770	57.381482	65.555137
1520.074300	68.529803	65.560142
1519.380845	49.505935	65.565146
1518.295792	58.401768	65.570151
1517.608493	57.993782	65.575156
1517.174987	57.856120	65.580161
1516.863052	57.233957	65.585166
1516.025051	57.397100	65.590170
1515.050915	54.677228	65.595175
1514.403122	52.154654	65.600180
1514.154492	62.994365	65.605185
1513.362625	60.929906	65.610190
1512.555154	54.588226	65.615194
1511.583320	61.450799	65.620199
1511.164662	61.807501	65.625204
1510.960483	57.438853	65.630209
1510.106605	54.403419	65.635214
1509.457587	57.496373	65.640218
1508.504739	61.689395	65.645223
1508.305902	53.576344	65.650228
1507.184675	57.833966	65.655233
1506.456283	53.367271	65.660238
1506.149367	52.624467	65.665242
1505.523723	59.425725	65.670247
1504.775197	55.069458	65.675252
1503.799086	66.631870	65.680257
1502.970727	56.647722	65.685262
1502.441487	51.450819	65.690266
1502.050740	52.380232	65.695271
1501.681806	58.117294	65.700276
1500.697181	55.928932	65.705281
1499.782093	58.851285	65.710286
1499.372890	47.419181	65.715290
1498.749083	60.792655	65.720295
1498.480156	52.782203	65.725300
1497.456283	63.551139	65.730305
1496.880595	61.121187	65.735310
1496.433672	50.382602	65.740314
1494.940176	80.193101	65.745319
1494.542526	59.964784	65.750324
1494.143924	48.628763	65.755329
1493.507621	58.009942	65.760334
1493.454452	65.647455	65.765338
1492.037834	62.174760	65.770343
1491.421356	54.563298	65.775348
1490.759447	50.015085	65.780353
1490.193990	55.706106	65.785358
1489.403572	51.033238	65.790362
1488.529279	59.895591	65.795367
1488.171516	53.723728	65.800372
1487.672014	57.540377	65.805377
1486.702950	46.195664	65.810382
1485.947711	63.953299	65.815386
1485.263564	55.907905	65.820391
1484.876692	42.352911	65.825396
1484.705003	52.727818	65.830401
1483.522078	50.853239	65.835406
1483.245173	40.084496	65.840410
1482.525066	54.900359	65.845415
1481.827550	56.588126	65.850420
1480.718158	59.369479	65.855425
1480.324653	60.226797	65.860430
1480.074755	53.842259	65.865434
1478.557942	56.574817	65.870439
1477.868298	41.402734	65.875444
1477.199411	61.176110	65.880449
1477.023315	54.043434	65.885454
1476.758499	44.832319	65.890458
1475.451500	46.776203	65.895463
1474.970043	54.962720	65.900468
1474.512095	59.176454	65.905473
1473.864257	54.526664	65.910478
1472.789077	52.721698	65.915482
1471.942816	53.392352	65.920487
1471.636239	50.389806	65.925492
1471.139731	42.934328	65.930497
1470.621477	46.093238	65.935502
1469.526500	51.365376	65.940506
1468.609504	68.037011	65.945511
1468.397695	41.821677	65.950516
1467.954686	43.907379	65.955521
1466.884849	67.577912	65.960526
1466.683159	51.472028	65.965530
1465.350582	49.504548	65.970535
1465.112023	70.031116	65.975540
1464.594629	33.455256	65.980545
1463.320667	71.131101	65.985550
1462.969090	48.241571	65.990554
1462.129569	67.330891	65.995559
1462.445046	56.179432	66.000564
1461.522704	43.177875	66.005569
1460.639185	53.874050	66.010574
1460.195164	54.428749	66.015578
1459.009899	44.009355	66.020583
1458.054195	40.644783	66.025588
1457.380799	54.983312	66.030593
1456.796800	57.953985	66.035598
1456.405073	35.747346	66.040602
1455.943991	62.791879	66.045607
1455.270049	28.964216	66.050612
1454.211039	66.154899	66.055617
1453.847294	43.126970	66.060622
1453.211541	53.812157	66.065626
1452.561193	58.699843	66.070631
1451.571747	47.593343	66.075636
1451.010957	52.656023	66.080641
1450.657731	60.850551	66.085646
1450.335097	56.814538	66.090650
1449.054310	71.527141	66.095655
1448.780238	51.608786	66.100660
1448.110011	43.223745	66.105665
1447.208208	51.355642	66.110670
1446.500167	46.307014	66.115674
1445.709319	57.551420	66.120679
1445.355246	50.920103	66.125684
1444.768236	48.603924	66.130689
1443.598352	48.576991	66.135694
1443.043495	44.699308	66.140698
1442.464691	46.092261	66.145703
1442.118661	48.998311	66.150708
1441.549035	51.378520	66.155713
1440.030420	53.755006	66.160718
1440.093005	52.277002	66.165722
1439.432533	53.988853	66.170727
1439.210516	38.349828	66.175732
1438.361001	45.502047	66.180737
1437.291783	53.688938	66.185742
1437.381199	52.495241	66.190746
1436.048021	43.799260	66.195751
1435.104392	49.052089	66.200756
1434.690963	48.658947	66.205761
1433.270703	52.232439	66.210766
1433.198363	51.111756	66.215770
1432.263637	52.208051	66.220775
1431.955096	47.352972	66.225780
1431.574896	49.349854	66.230785
1430.987363	55.356618	66.235790
1430.376437	44.089054	66.240794
1429.149964	43.151791	66.245799
1428.961103	62.897767	66.250804
1428.503899	54.426834	66.255809
1427.193846	56.722876	66.260814
1426.307466	29.285463	66.265818
1425.958263	67.452976	66.270823
1425.860756	43.066037	66.275828
1424.961037	52.599468	66.280833
1423.909351	64.148678	66.285838
1423.422648	47.679689	66.290842
1422.890214	52.745751	66.295847
1422.122410	67.731635	66.300852
1421.317537	43.373541	66.305857
1420.270550	54.046821	66.310862
1420.457227	59.905315	66.315866
1419.944528	51.212979	66.320871
1419.183955	31.078678	66.325876
1418.379854	58.915700	66.330881
1417.517655	63.149537	66.335886
1416.473445	47.951827	66.340890
1415.703411	62.647912	66.345895
1415.267135	46.722826	66.350900
1415.185354	57.439822	66.355905
1414.304291	62.998097	66.360910
1414.304388	42.687698	66.365914
1412.674383	46.840140	66.370919
1412.195960	56.338158	66.375924
1411.583918	58.671500	66.380929
1410.903398	44.450439	66.385934
1410.190091	37.119320	66.390938
1409.409839	52.465123	66.395943
1409.176591	54.539574	66.400948
1408.369765	46.901627	66.405953
1407.068149	47.863861	66.410958
1406.741984	49.331782	66.415962
1406.444065	59.477603	66.420967
1405.766963	49.419002	66.425972
1404.789008	50.556869	66.430977
1404.123265	52.446179	66.435982
1404.051538	47.939806	66.440986
1403.440675	51.021987	66.445991
1402.125826	62.802255	66.450996
1401.573724	42.600122	66.456001
1400.849029	56.938927	66.461006
1400.323865	47.398633	66.466010
1399.784550	55.581738	66.471015
1399.094661	43.243409	66.476020
1398.543695	48.003348	66.481025
1397.822605	58.762030	66.486030
1396.982817	45.977609	66.491034
1395.912072	51.998102	66.496039
1395.476080	53.101872	66.501044
1395.207603	45.958664	66.506049
1394.558685	57.150560	66.511054
1394.087264	48.691361	66.516058
1393.388251	48.980682	66.521063
1392.757659	48.541640	66.526068
1391.355758	49.751624	66.531073
1390.854395	51.950689	66.536078
1390.277406	44.722482	66.541082
1389.791694	48.018154	66.546087
1389.566951	50.277328	66.551092
1388.220239	47.285578	66.556097
1387.354428	56.036223	66.561102
1387.488033	44.888449	66.566106
1386.789231	49.867422	66.571111
1385.752308	48.165220	66.576116
1384.971856	49.139244	66.581121
1384.203418	41.216098	66.586126
1384.268122	35.869637	66.591130
1383.239363	37.949107	66.596135
1382.283018	48.748331	66.601140
1381.893265	46.823424	66.606145
1381.374498	53.123606	66.611150
1380.577961	39.442955	66.616154
1379.264273	54.750552	66.621159
1378.828537	43.146091	66.626164
1378.773400	50.105836	66.631169
1378.122878	48.963518	66.636174
1377.401627	37.806550	66.641178
1376.369054	45.740059	66.646183
1375.665196	43.584391	66.651188
1375.539803	63.992030	66.656193
1374.624063	48.070628	66.661198
1373.827282	39.778267	66.666202
1373.084434	50.838440	66.671207
1372.782541	50.992108	66.676212
1372.367712	68.501695	66.681217
1371.114853	35.160312	66.686222
1370.422661	50.090013	66.691226
1369.867194	46.341751	66.696231
1369.597488	49.196254	66.701236
1368.622197	48.545513	66.706241
1367.720752	40.793319	66.711246
1367.484909	40.084967	66.716250
1366.830374	59.983792	66.721255
1366.077860	52.885986	66.726260
1365.239612	43.641466	66.731265
1364.264282	54.875785	66.736270
1364.170788	50.524256	66.741274
1363.252061	54.122142	66.746279
1362.403295	49.680936	66.751284
1362.388627	39.969633	66.756289
1361.448085	58.660288	66.761294
1360.808935	42.270751	66.766298
1359.890990	52.776885	66.771303
1359.654142	42.452793	66.776308
1358.834811	57.919933	66.781313
1358.060116	58.459404	66.786318
1357.305886	55.274150	66.791322
1356.665606	53.024805	66.796327
1356.502856	46.367829	66.801332
1355.676566	50.089789	66.806337
1354.440695	49.515164	66.811342
1354.318138	57.592609	66.816346
1353.164594	48.842892	66.821351
1352.794103	56.292719	66.826356
1352.402766	31.477883	66.831361
1351.382084	72.508529	66.836366
1350.926955	38.970969	66.841370
1350.501426	16.996847	66.846375
1349.775877	18.771097	66.851380
1349.157402	63.503401	66.856385
1347.413183	58.999539	66.861390
1346.797414	48.196379	66.866394
1346.538649	28.963181	66.871399
1346.262848	73.355627	66.876404
1346.191304	40.104011	66.881409
1345.180483	74.940639	66.886414
1344.403698	42.808757	66.891418
1343.333165	48.502816	66.896423
1342.917185	62.306877	66.901428
1342.496791	54.907136	66.906433
1341.369417	48.807180	66.911438
1340.930129	53.926255	66.916442
1340.517696	54.308803	66.921447
1339.544576	52.538132	66.926452
1338.624933	42.275274	66.931457
1338.001779	70.614969	66.936462
1337.863653	46.516772	66.941466
1337.053324	47.298448	66.946471
1336.082785	54.052058	66.951476
1335.610993	53.898436	66.956481
1334.703373	43.433402	66.961486
1334.694971	55.846501	66.966490
1333.471775	49.369134	66.971495
1332.762975	49.453453	66.976500
1332.480818	40.292434	66.981505
1331.794823	73.391725	66.986510
1331.328428	41.530625	66.991514
1330.147358	41.309987	66.996519
1329.539978	62.540103	67.001524
1329.336031	30.958995	67.006529
1328.371757	67.967471	67.011534
1327.496980	35.084824	67.016538
1327.196201	64.071822	67.021543
1326.354053	39.402760	67.026548
1325.897913	56.491560	67.031553
1324.876239	36.096043	67.036558
1324.050555	54.060414	67.041562
1323.775606	53.217939	67.046567
1323.025581	37.128313	67.051572
1322.315575	64.532512	67.056577
1321.654850	52.601140	67.061582
1320.976418	37.135623	67.066586
1320.397205	59.132357	67.071591
1320.180223	21.912793	67.076596
1319.319176	63.750634	67.081601
1318.466454	30.386699	67.086606
1317.734933	60.676868	67.091610
1316.554290	50.067590	67.096615
1315.928170	62.596235	67.101620
1316.000424	45.145910	67.106625
1315.057775	56.345087	67.111630
1315.147797	49.157518	67.116634
1313.891560	49.002450	67.121639
1312.918651	60.211171	67.126644
1312.691840	49.678915	67.131649
1311.994019	43.826069	67.136654
1311.246554	42.549375	67.141658
1310.371868	62.992540	67.146663
1310.103893	49.765607	67.151668
1309.452761	39.501079	67.156673
1308.235613	48.369089	67.161678
1308.125420	42.110604	67.166682
1307.302286	48.924363	67.171687
1306.443299	38.181966	67.176692
1305.776929	52.273395	67.181697
1305.190644	58.431364	67.186702
1304.892519	36.369171	67.191706
1304.052367	54.744261	67.196711
1303.427608	44.844532	67.201716
1302.605927	43.921824	67.206721
1302.164459	53.147479	67.211726
1301.209910	45.339102	67.216730
1300.456573	51.807466	67.221735
1299.730387	46.887923	67.226740
1299.827114	43.158995	67.231745
1298.535933	49.067913	67.236750
1297.929454	44.971401	67.241754
1297.122004	46.083779	67.246759
1296.823359	48.383091	67.251764
1296.064653	49.389952	67.256769
1295.080305	53.334169	67.261774
1294.766117	50.066366	67.266778
1294.046407	42.816725	67.271783
1293.506207	49.864617	67.276788
1292.724428	40.623768	67.281793
1291.251787	60.084975	67.286798
1291.586488	47.115462	67.291802
1290.824131	34.489095	67.296807
1289.904935	53.166899	67.301812
1289.548075	31.541395	67.306817
1288.585876	60.240883	67.311822
1288.344149	46.347491	67.316826
1287.319887	42.691125	67.321831
1286.069883	48.967226	67.326836
1286.005313	57.879086	67.331841
1285.582095	51.306102	67.336846
1285.518192	49.912858	67.341850
1283.985905	42.756136	67.346855
1283.499350	58.425839	67.351860
1282.723214	50.015114	67.356865
1282.228773	46.039561	67.361870
1281.183285	44.253613	67.366874
1280.717561	50.061268	67.371879
1280.021838	49.331423	67.376884
1279.915876	45.371378	67.381889
1278.522464	51.561476	67.386894
1278.021084	35.817105	67.391898
1277.278569	62.015414	67.396903
1277.279193	59.512816	67.401908
1276.441747	39.343492	67.406913
1275.119148	56.010247	67.411918
1274.807604	47.568240	67.416922
1274.500067	41.729049	67.421927
1273.659054	57.967595	67.426932
1272.809884	53.116495	67.431937
1272.229379	51.967803	67.436942
1271.923310	39.576392	67.441946
1270.805122	52.030306	67.446951
1270.054938	54.590636	67.451956
1269.671167	34.790725	67.456961
1268.731458	66.173673	67.461966
1268.513052	46.117230	67.466970
1267.305160	45.221244	67.471975
1267.033270	60.979819	67.476980
1266.456237	28.587614	67.481985
1265.620883	57.388352	67.486990
1265.079257	38.886087	67.491994
1264.639527	43.180523	67.496999
1263.682089	34.568413	67.502004
1263.131170	72.905153	67.507009
1261.950333	62.682266	67.512014
1262.208397	28.815355	67.517018
1261.281776	55.310993	67.522023
1259.934518	40.793896	67.527028
1259.443926	63.325304	67.532033
1258.861858	46.045247	67.537038
1258.714632	48.258990	67.542042
1257.590806	46.496545	67.547047
1256.660106	53.199692	67.552052
1256.559762	49.429558	67.557057
1255.823268	57.383843	67.562062
1255.343765	43.930374	67.567066
1254.598646	45.758224	67.572071
1253.942241	46.982212	67.577076
1252.697080	45.138140	67.582081
1251.601276	56.125148	67.587086
1251.101435	48.112038	67.592090
1251.201018	49.917547	67.597095
1250.812538	43.528279	67.602100
1250.420207	38.640827	67.607105
1249.263978	56.962106	67.612110
1248.617674	44.158031	67.617114
1247.654685	45.984255	67.622119
1246.486623	54.395073	67.627124
1245.972025	61.956128	67.632129
1245.474974	41.694851	67.637134
1245.329353	56.983930	67.642138
1245.000919	34.592279	67.647143
1244.034941	49.038841	67.652148
1243.015979	55.197806	67.657153
1242.683607	52.407546	67.662158
1242.506106	39.815935	67.667162
1241.112570	49.861569	67.672167
1240.305116	60.775931	67.677172
1240.110628	43.574605	67.682177
1238.482391	62.401432	67.687182
1238.079791	55.162885	67.692186
1237.392303	37.325620	67.697191
1236.813529	60.415070	67.702196
1236.677646	44.238868	67.707201
1236.348361	39.273588	67.712206
1235.876149	60.714013	67.717210
1234.823174	45.410575	67.722215
1234.166535	52.705639	67.727220
1232.967000	50.133682	67.732225
1232.287952	46.800904	67.737230
1231.879851	47.925495	67.742234
1231.502230	46.225758	67.747239
1230.624164	53.964446	67.752244
1229.918217	57.340892	67.757249
1228.963166	64.060539	67.762254
1229.017388	36.711794	67.767258
1228.336356	40.749723	67.772263
1227.264764	54.981284	67.777268
1226.588483	34.493068	67.782273
1226.158667	64.828305	67.787278
1225.043371	36.918071	67.792282
1224.240851	52.884004	67.797287
1223.710979	46.553491	67.802292
1223.582636	31.979805	67.807297
1222.862654	69.681115	67.812302
1222.312997	32.640621	67.817306
1221.022573	58.937083	67.822311
1220.675124	47.487355	67.827316
1220.655606	37.726380	67.832321
1219.520798	66.079606	67.837326
1219.067637	34.585471	67.842330
1218.175109	57.543462	67.847335
1216.882217	51.097740	67.852340
1216.295729	51.320332	67.857345
1215.782711	51.083405	67.862350
1215.304044	59.493424	67.867354
1215.393686	42.261120	67.872359
1213.896989	51.725529	67.877364
1213.601469	47.704170	67.882369
1212.677525	52.051956	67.887374
1212.542735	41.691168	67.892378
1211.341879	61.842444	67.897383
1210.560191	35.836100	67.902388
1210.053990	52.551246	67.907393
1209.612277	42.155686	67.912398
1209.018351	35.737600	67.917402
1208.175105	59.053596	67.922407
1207.381504	55.459929	67.927412
1207.268643	42.224134	67.932417
1206.059082	46.530607	67.937422
1205.246174	34.434267	67.942426
1204.642937	49.583220	67.947431
1204.503874	39.514838	67.952436
1203.701872	43.109980	67.957441
1202.755213	47.297383	67.962446
1202.396584	42.950184	67.967450
1201.681853	40.039391	67.972455
1200.517055	62.670116	67.977460
1200.256106	27.365631	67.982465
1199.240247	65.227510	67.987470
1199.136055	45.679610	67.992474
1198.355176	41.465785	67.997479
1197.253797	50.403735	68.002484
1196.954821	36.194639	68.007489
1196.451562	55.337731	68.012494
1196.317746	22.471419	68.017498
1194.891490	56.792192	68.022503
1194.337162	36.913775	68.027508
1193.610688	56.193284	68.032513
1192.340788	30.122675	68.037518
1191.770560	67.167828	68.042522
1191.757175	38.834821	68.047527
1191.181827	55.158859	68.052532
1190.958484	28.538650	68.057537
1189.506245	38.535289	68.062542
1188.966051	52.382747	68.067546
1188.840131	44.097317	68.072551
1187.553044	34.848561	68.077556
1186.816507	48.995310	68.082561
1186.141064	51.692005	68.087566
1185.821899	40.247256	68.092570
1184.988518	56.877245	68.097575
1183.826266	40.569393	68.102580
1183.536419	54.056935	68.107585
1182.747937	58.402113	68.112590
1182.427260	30.065955	68.117594
1182.060771	48.854566	68.122599
1181.731937	49.599144	68.127604
1180.838491	41.494113	68.132609
1179.271073	57.141739	68.137614
1178.697554	32.385907	68.142618
1178.520812	47.873875	68.147623
1177.848801	65.244583	68.152628
1177.616508	38.600553	68.157633
1176.650440	62.560537	68.162638
1176.311938	35.253762	68.167642
1175.294937	62.104399	68.172647
1174.146812	34.423347	68.177652
1173.797222	49.309624	68.182657
1173.213563	39.952167	68.187662
1172.444362	35.604037	68.192666
1171.444469	46.482775	68.197671
1171.110049	60.680703	68.202676
1170.711499	26.558709	68.207681
1170.046818	57.025883	68.212686
1169.330913	32.004129	68.217690
1168.497426	58.849231	68.222695
1167.797321	40.854735	68.227700
1167.867070	32.054093	68.232705
1166.477547	58.208635	68.237710
1165.902947	32.079509	68.242714
1165.165526	58.264386	68.247719
1164.273562	37.553461	68.252724
1163.427253	43.632954	68.257729
1162.598431	43.034691	68.262734
1162.258082	24.771704	68.267738
1162.080054	52.143313	68.272743
1161.274170	27.946401	68.277748
1161.436400	57.924121	68.282753
1160.061409	39.253242	68.287758
1159.587317	28.640514	68.292762
1158.535240	38.871562	68.297767
1157.545953	54.260104	68.302772
1157.104508	51.766314	68.307777
1156.353890	39.209095	68.312782
1156.645633	17.179330	68.317786
1155.604928	56.021229	68.322791
1154.287092	56.074725	68.327796
1154.096057	31.980296	68.332801
1153.380142	21.341380	68.337806
1152.508476	70.893467	68.342810
1151.433543	54.552811	68.347815
1151.217881	23.829910	68.352820
1150.865317	58.782580	68.357825
1150.297234	33.404602	68.362830
1149.381799	60.166549	68.367834
1149.267477	32.508761	68.372839
1147.967718	53.547789	68.377844
1147.148967	35.356145	68.382849
1146.402056	48.213076	68.387854
1146.146273	40.534909	68.392858
1145.747085	51.444276	68.397863
1144.908256	46.982652	68.402868
1143.912439	27.846237	68.407873
1143.402469	61.776892	68.412878
1143.063973	43.876277	68.417882
1142.065265	39.664001	68.422887
1141.026321	55.574511	68.427892
1140.917216	34.881022	68.432897
1140.077233	50.780384	68.437902
1139.727449	20.285399	68.442906
1138.813233	55.209114	68.447911
1138.067874	28.646714	68.452916
1137.830851	47.034700	68.457921
1136.493372	34.402100	68.462926
1135.707894	54.410056	68.467930
1135.892772	22.789288	68.472935
1135.043850	44.232826	68.477940
1134.506754	60.512944	68.482945
1133.577407	23.097694	68.487950
1133.178430	46.738818	68.492954
1132.229639	29.515582	68.497959
1131.235603	55.479501	68.502964
1130.780596	47.669022	68.507969
1130.309060	42.623886	68.512974
1129.942271	40.409954	68.517978
1129.016298	47.443530	68.522983
1128.025502	41.301465	68.527988
1127.854922	50.022019	68.532993
1126.652739	37.399443	68.537998
1126.050383	41.205695	68.543002
1125.575051	43.175168	68.548007
1124.938437	47.527743	68.553012
1124.748180	26.035079	68.558017
1123.281524	62.647214	68.563022
1123.114610	43.541380	68.568026
1122.659453	30.429434	68.573031
1121.130473	53.201657	68.578036
1120.691271	47.487508	68.583041
1120.171612	34.338512	68.588046
1119.748493	41.393033	68.593050
1119.674904	51.080564	68.598055
1118.463317	39.200625	68.603060
1117.954498	47.389947	68.608065
1117.059850	50.403785	68.613070
1116.110005	41.755841	68.618074
1115.504304	31.517280	68.623079
1114.897515	34.069034	68.628084
1114.672325	51.914268	68.633089
1113.861875	49.299411	68.638094
1113.161659	36.234323	68.643098
1112.615763	35.652577	68.648103
1111.544479	60.056635	68.653108
1110.693312	26.957526	68.658113
1109.744827	37.355030	68.663118
1109.231249	44.140101	68.668122
1109.073663	49.916113	68.673127
1108.790602	47.783480	68.678132
1108.277609	32.028408	68.683137
1106.690806	44.881737	68.688142
1106.503621	39.815035	68.693146
1106.256092	43.260516	68.698151
1105.342406	50.482950	68.703156
1104.640666	44.126192	68.708161
1104.141887	40.892511	68.713166
1102.668514	34.175960	68.718170
1102.109418	52.419640	68.723175
1101.459827	48.134506	68.728180
1101.532418	36.837198	68.733185
1100.731753	44.265571	68.738190
1099.632356	58.189367	68.743194
1098.956359	41.954033	68.748199
1098.087359	37.852028	68.753204
1098.168376	29.874312	68.758209
1097.235195	41.966120	68.763214
1096.502013	39.998120	68.768218
1096.110063	45.106537	68.773223
1095.307122	41.181675	68.778228
1094.461408	38.957196	68.783233
1093.846174	41.453531	68.788238
1093.333735	33.608051	68.793242
1093.155126	37.851513	68.798247
1091.824943	38.342227	68.803252
1091.363325	39.511619	68.808257
1090.767001	44.931652	68.813262
1089.982722	32.576934	68.818266
1089.409837	37.141717	68.823271
1088.382314	38.823727	68.828276
1088.184983	37.412293	68.833281
1087.064312	29.892209	68.838286
1086.405765	37.430436	68.843290
1085.753126	38.496177	68.848295
1085.293951	50.843747	68.853300
1084.837443	41.210638	68.858305
1083.747671	40.742213	68.863310
1082.959646	40.312523	68.868314
1082.816450	41.033892	68.873319
1082.012889	40.023224	68.878324
1081.704918	34.266140	68.883329
1080.388291	48.413711	68.888334
1080.108037	43.357084	68.893338
1079.728710	28.790240	68.898343
1078.649687	44.888469	68.903348
1077.862895	45.109839	68.908353
1077.368598	46.987724	68.913358
1076.900311	36.063445	68.918362
1076.001365	33.003806	68.923367
1075.308033	40.120233	68.928372
1074.938402	42.437163	68.933377
1074.120762	52.928988	68.938382
1073.162233	49.850439	68.943386
1072.633867	38.415343	68.948391
1071.662424	49.352660	68.953396
1071.608600	34.078051	68.958401
1071.151626	47.492822	68.963406
1070.387129	38.126319	68.968410
1069.497978	27.713676	68.973415
1068.736282	51.234308	68.978420
1067.740868	46.567394	68.983425
1067.148660	31.059896	68.988430
1066.595021	39.395114	68.993434
1066.388799	38.513354	68.998439
1065.874771	33.851872	69.003444
1065.053650	25.572977	69.008449
1064.312935	47.035583	69.013454
1063.926358	42.904159	69.018458
1062.795728	24.175580	69.023463
1061.506582	40.879643	69.028468
1061.274270	39.331856	69.033473
1060.525073	37.796905	69.038478
1060.670997	37.223391	69.043482
1059.669251	34.197456	69.048487
1058.979056	39.160935	69.053492
1058.523829	35.762649	69.058497
1057.573094	42.073237	69.063502
1056.551615	37.432554	69.068506
1056.370633	42.250383	69.073511
1055.893829	51.763938	69.078516
1054.877740	40.212470	69.083521
1053.992698	41.666833	69.088526
1053.506439	35.209592	69.093530
1053.340995	39.376848	69.098535
1052.309214	46.682732	69.103540
1051.484298	41.186070	69.108545
1050.626148	39.660569	69.113550
1050.282255	39.573384	69.118554
1049.894642	43.258763	69.123559
1048.947186	40.979523	69.128564
1048.621246	29.162173	69.133569
1047.881907	38.156110	69.138574
1046.962667	32.116240	69.143578
1046.575596	40.559000	69.148583
1045.344781	45.811902	69.153588
1045.062431	28.577316	69.158593
1044.141707	41.513942	69.163598
1043.327195	34.553856	69.168602
1042.725807	46.107219	69.173607
1042.268238	46.960598	69.178612
1042.172481	39.575527	69.183617
1041.253469	44.999594	69.188622
1040.439596	43.282557	69.193626
1040.132677	41.642565	69.198631
1038.793896	37.388242	69.203636
1037.984247	42.900564	69.208641
1037.519713	41.340836	69.213646
1037.014079	46.393231	69.218650
1037.135893	40.253983	69.223655
1035.846491	34.208347	69.228660
1035.184047	43.073368	69.233665
1034.640795	37.721134	69.238670
1033.795988	43.970726	69.243674
1032.997519	38.774204	69.248679
1032.202393	53.876430	69.253684
1031.975827	25.142193	69.258689
1031.571436	35.153554	69.263694
1030.371966	41.976785	69.268698
1029.997572	36.848415	69.273703
1028.981300	55.555896	69.278708
1028.537153	35.522838	69.283713
1027.840841	58.649899	69.288718
1027.317028	36.257871	69.293722
1026.638123	56.520110	69.298727
1025.492226	41.606880	69.303732
1024.375024	48.166303	69.308737
1024.390499	34.916441	69.313742
1023.930769	49.030215	69.318746
1023.742358	19.405288	69.323751
1022.329074	47.263509	69.328756
1022.236355	32.824541	69.333761
1021.357094	33.880619	69.338766
1020.669150	48.711912	69.343770
1019.843793	31.188415	69.348775
1018.942690	44.334808	69.353780
1018.644771	37.171128	69.358785
1018.240253	41.250267	69.363790
1017.419078	41.529162	69.368794
1016.608341	41.461058	69.373799
1015.791930	43.814380	69.378804
1015.259095	49.386748	69.383809
1014.573195	46.326352	69.388814
1013.850854	34.171538	69.393818
1013.451582	38.361801	69.398823
1012.898332	47.053345	69.403828
1011.919915	41.986378	69.408833
1011.282013	43.524436	69.413838
1010.644141	41.311074	69.418842
1010.479725	28.539251	69.423847
1009.266594	46.445446	69.428852
1009.090938	35.867280	69.433857
1008.024034	49.897883	69.438862
1007.004757	30.736896	69.443866
1006.615488	55.046652	69.448871
1005.807199	40.237415	69.453876
1005.678693	37.991904	69.458881
1004.895808	53.336604	69.463886
1004.282734	38.947302	69.468890
1003.583467	27.160974	69.473895
1002.715910	45.292878	69.478900
1001.873136	45.050111	69.483905
1001.314468	44.706954	69.488910
1000.553461	31.886546	69.493914
1000.455891	31.006429	69.498919
999.494682	44.521918	69.503924
999.346785	46.934464	69.508929
998.466343	41.345735	69.513934
997.130455	38.275217	69.518938
996.484306	38.190397	69.523943
995.784479	40.917821	69.528948
995.804411	32.661258	69.533953
995.262852	39.821361	69.538958
994.020978	43.361967	69.543962
993.343405	32.174558	69.548967
992.650749	35.190988	69.553972
992.311031	37.656126	69.558977
991.162883	46.997382	69.563982
990.716863	44.833924	69.568986
990.324515	34.925722	69.573991
989.806313	50.627263	69.578996
989.054496	37.583051	69.584001
988.034015	43.338654	69.589006
987.244616	40.882913	69.594010
987.350061	26.712040	69.599015
985.869835	29.819079	69.604020
985.162798	34.279072	69.609025
984.921448	36.111998	69.614030
984.211732	42.783215	69.619034
983.843792	37.962898	69.624039
983.148650	36.780479	69.629044
982.198106	37.411113	69.634049
981.951242	50.079709	69.639054
981.064936	35.618778	69.644058
980.281718	27.567267	69.649063
979.434528	49.064165	69.654068
979.300834	29.369656	69.659073
977.773769	36.811127	69.664078
977.200928	39.545160	69.669082
976.859534	37.808164	69.674087
976.320698	36.629263	69.679092
976.127984	38.979555	69.684097
975.093421	30.980648	69.689102
973.898552	48.891835	69.694106
973.968733	30.644009	69.699111
972.979025	52.384352	69.704116
972.203435	40.882970	69.709121
971.446998	24.477592	69.714126
970.776148	55.204337	69.719130
970.714738	32.333512	69.724135
969.951195	30.417690	69.729140
969.061993	30.354201	69.734145
968.541954	28.560480	69.739150
968.060049	32.043256	69.744154
967.564207	38.101730	69.749159
966.209411	48.685345	69.754164
965.806660	33.630270	69.759169
965.082905	43.796527	69.764174
963.885302	34.454826	69.769178
963.920495	33.359631	69.774183
963.228033	42.489625	69.779188
963.063631	39.678996	69.784193
961.955108	35.096358	69.789198
960.958712	37.429449	69.794202
960.552591	42.958008	69.799207
959.394563	32.438388	69.804212
958.601273	34.275559	69.809217
958.229940	43.974177	69.814222
957.786136	39.851881	69.819226
957.427881	32.830274	69.824231
956.746927	48.679129	69.829236
955.874669	46.562996	69.834241
954.755314	44.265415	69.839246
954.558396	42.524358	69.844250
954.432804	28.521129	69.849255
953.317058	47.353246	69.854260
953.060932	44.461020	69.859265
952.107757	23.436718	69.864270
950.676348	41.547957	69.869274
950.394084	38.090636	69.874279
950.016828	34.545933	69.879284
949.296709	54.161899	69.884289
948.418270	42.323667	69.889294
947.612422	46.595977	69.894298
947.279806	30.435392	69.899303
947.022184	43.425799	69.904308
945.879204	44.276293	69.909313
945.461274	43.661608	69.914318
944.752116	46.705907	69.919322
943.943628	41.414822	69.924327
943.128502	46.805044	69.929332
942.646873	41.353146	69.934337
942.060283	45.366652	69.939342
941.277758	38.461436	69.944346
940.689853	43.858080	69.949351
939.792255	46.298456	69.954356
939.374026	45.546630	69.959361
938.833270	35.758245	69.964366
937.962551	51.881718	69.969370
937.363324	44.786492	69.974375
936.943248	40.663579	69.979380
936.166192	37.261336	69.984385
935.187792	36.097195	69.989390
934.390807	54.252582	69.994394
934.182511	45.075161	69.999399
933.740052	35.326328	70.004404
933.033718	44.691915	70.009409
931.773194	31.616720	70.014414
931.609856	46.410275	70.019418
930.494549	37.664176	70.024423
929.502859	41.248576	70.029428
929.241066	55.665162	70.034433
928.506529	28.692751	70.039438
928.150165	43.644745	70.044442
928.183088	14.457714	70.049447
926.985825	61.333523	70.054452
926.507317	32.700902	70.059457
925.506128	58.755869	70.064462
924.386414	27.101475	70.069466
923.882004	56.267426	70.074471
923.243610	46.814683	70.079476
923.376090	28.074429	70.084481
922.426795	34.242906	70.089486
921.674743	53.025051	70.094490
921.472059	27.958046	70.099495
920.079125	58.086942	70.104500
918.973912	27.395299	70.109505
918.685532	59.259621	70.114510
918.435881	38.005104	70.119514
917.693918	35.354190	70.124519
916.703874	50.179952	70.129524
916.259007	38.607048	70.134529
915.921223	36.576187	70.139534
914.681627	45.176692	70.144538
914.571257	11.259740	70.149543
913.389417	42.359488	70.154548
913.042642	24.920742	70.159553
911.802123	37.428909	70.164558
911.220005	44.136605	70.169562
910.706224	41.846757	70.174567
910.341440	31.312899	70.179572
910.080747	44.734285	70.184577
909.330324	32.106189	70.189582
908.176590	38.609966	70.194586
907.999549	45.164899	70.199591
907.055671	30.312643	70.204596
906.073706	45.372074	70.209601
905.960676	29.091409	70.214606
904.854981	24.022673	70.219610
904.191190	27.236371	70.224615
903.277512	44.520956	70.229620
902.876594	36.864355	70.234625
902.676191	21.363970	70.239630
901.713880	48.090793	70.244634
901.426441	22.971062	70.249639
900.606419	23.808028	70.254644
899.856890	41.418134	70.259649
898.610209	40.583691	70.264654
898.180624	12.744397	70.269658
897.795713	52.530549	70.274663
897.307696	19.313897	70.279668
896.394871	52.674687	70.284673
896.000903	32.047099	70.289678
895.100407	35.620153	70.294682
894.414732	36.227593	70.299687
893.296385	43.056892	70.304692
892.319230	25.029368	70.309697
892.338979	66.460504	70.314702
891.892215	46.763778	70.319706
891.763390	47.020843	70.324711
890.638855	39.164019	70.329716
890.324273	34.202772	70.334721
889.428302	24.797353	70.339726
887.996377	44.064555	70.344730
887.619238	38.753733	70.349735
887.100144	32.293878	70.354740
886.818977	15.019746	70.359745
885.822700	58.162616	70.364750
884.819487	31.512090	70.369754
884.578419	42.453064	70.374759
884.024017	31.435324	70.379764
883.265435	33.244917	70.384769
882.723420	45.476370	70.389774
882.075135	40.804760	70.394778
881.698952	34.069862	70.399783
880.257665	39.843583	70.404788
879.467462	31.525151	70.409793
879.454835	28.718762	70.414798
878.431078	33.268605	70.419802
877.536633	32.173124	70.424807
876.665769	43.543893	70.429812
876.728191	40.695598	70.434817
876.333260	30.265891	70.439822
875.488426	38.038796	70.444826
874.760999	34.723291	70.449831
874.161628	37.538832	70.454836
873.331679	41.311970	70.459841
872.317229	44.184108	70.464846
871.616396	50.018188	70.469850
871.465578	31.737744	70.474855
870.895616	30.787737	70.479860
870.370382	36.199647	70.484865
869.592520	36.451197	70.489870
868.638850	48.581016	70.494874
867.847406	33.597292	70.499879
866.721123	35.485906	70.504884
866.015158	51.611554	70.509889
865.947748	18.152952	70.514894
865.457917	36.666278	70.519898
865.114337	33.726486	70.524903
863.919003	47.616722	70.529908
863.373991	29.913081	70.534913
863.111164	28.168331	70.539918
862.269442	31.350435	70.544922
861.788542	40.057286	70.549927
860.888270	31.896721	70.554932
860.236119	32.006848	70.559937
859.176704	29.034330	70.564942
858.323299	28.952569	70.569946
858.336255	36.803419	70.574951
857.397630	32.433481	70.579956
856.345474	29.614344	70.584961
855.896154	26.328700	70.589966
855.136977	57.689214	70.594970
854.856098	27.732140	70.599975
854.457783	41.057155	70.604980
853.913097	46.390168	70.609985
853.008335	32.760108	70.614990
852.362183	33.720799	70.619994
851.327269	28.306524	70.624999
850.331597	30.152282	70.630004
849.923185	29.149763	70.635009
849.658525	21.575572	70.640014
848.853161	27.853620	70.645018
848.159125	32.220116	70.650023
847.697641	42.464495	70.655028
847.098242	29.446557	70.660033
846.180783	30.183935	70.665038
845.154184	41.888564	70.670042
844.725179	28.878200	70.675047
844.096162	44.698296	70.680052
843.740720	38.814774	70.685057
842.516411	33.894248	70.690062
841.672051	41.266559	70.695066
841.574403	27.708319	70.700071
841.146361	39.196265	70.705076
840.994366	37.575797	70.710081
840.009321	33.317329	70.715086
838.977831	45.092124	70.720090
838.691738	47.791585	70.725095
837.621456	44.248395	70.730100
837.159676	29.056110	70.735105
836.369245	27.642906	70.740110
835.382943	37.690125	70.745114
834.918389	32.889947	70.750119
834.466950	25.512634	70.755124
833.625140	41.448592	70.760129
833.141985	33.961211	70.765134
832.358844	43.769528	70.770138
832.083212	20.759398	70.775143
830.850855	45.485564	70.780148
830.203676	45.691097	70.785153
829.624530	26.807089	70.790158
828.864300	41.454366	70.795162
828.711105	36.733937	70.800167
827.618209	50.283045	70.805172
826.801746	36.522252	70.810177
826.499047	44.661452	70.815182
825.881207	43.671769	70.820186
825.147850	31.220760	70.825191
824.302920	37.148740	70.830196
823.781047	48.856623	70.835201
823.543410	23.881953	70.840206
822.246446	49.045745	70.845210
821.812250	40.307985	70.850215
821.210276	42.482161	70.855220
820.584845	23.392649	70.860225
819.553877	40.774756	70.865230
818.479282	42.759239	70.870234
818.600059	36.670623	70.875239
818.254116	33.787982	70.880244
817.117439	31.054852	70.885249
816.652222	34.763644	70.890254
815.828935	46.264045	70.895258
814.989998	39.495584	70.900263
814.025675	38.706126	70.905268
813.619697	29.243248	70.910273
813.321209	21.165116	70.915278
812.719810	54.634029	70.920282
812.393668	34.121826	70.925287
811.371393	38.425464	70.930292
811.096596	36.447669	70.935297
809.835659	26.961609	70.940302
808.628398	31.255268	70.945306
808.361096	27.808204	70.950311
808.003423	26.684081	70.955316
807.044068	50.549983	70.960321
806.554392	25.922924	70.965326
805.485075	38.589952	70.970330
805.270617	39.057761	70.975335
805.025299	41.828002	70.980340
804.298688	35.382276	70.985345
803.360542	34.561848	70.990350
802.506121	34.082893	70.995354
801.904253	36.227095	71.000359
800.872188	35.727532	71.005364
799.994042	37.881018	71.010369
800.026599	33.307638	71.015374
799.529591	42.054905	71.020378
799.225380	34.053370	71.025383
798.018649	38.920936	71.030388
797.533273	36.229219	71.035393
796.688527	37.201035	71.040398
795.959854	41.355449	71.045402
795.373946	26.771117	71.050407
794.968980	38.085087	71.055412
794.315996	37.468421	71.060417
793.337274	29.085419	71.065422
792.545031	30.805783	71.070426
792.373489	34.191879	71.075431
791.120683	33.642305	71.080436
790.548575	35.223555	71.085441
789.987338	43.796553	71.090446
789.418479	45.399364	71.095450
788.988866	28.645593	71.100455
787.771853	34.413621	71.105460
787.514027	32.723275	71.110465
787.428382	29.442833	71.115470
786.002113	36.204492	71.120474
785.225786	34.863172	71.125479
784.991646	35.569072	71.130484
784.238690	33.397746	71.135489
783.183630	38.312135	71.140494
782.633226	50.270558	71.145498
782.260654	31.080882	71.150503
781.784364	38.167548	71.155508
780.759858	31.386068	71.160513
780.054571	27.400050	71.165518
779.235707	44.880866	71.170522
778.950431	36.655556	71.175527
777.869686	36.102253	71.180532
777.023401	34.653806	71.185537
777.029280	34.690747	71.190542
776.085123	39.560679	71.195546
775.747266	29.530328	71.200551
774.908141	38.240595	71.205556
774.098942	43.593648	71.210561
773.932902	43.615380	71.215566
772.885486	30.897432	71.220570
772.159654	48.224679	71.225575
771.425535	38.609045	71.230580
771.063812	42.536328	71.235585
770.517135	30.404118	71.240590
769.211736	45.653829	71.245594
768.808252	27.680130	71.250599
768.259840	41.647177	71.255604
767.825009	42.779246	71.260609
767.048738	42.748312	71.265614
766.078185	49.446906	71.270618
765.808197	32.915300	71.275623
765.128545	37.118684	71.280628
764.139292	32.668540	71.285633
763.853532	35.103036	71.290638
763.180955	42.179953	71.295642
762.729211	35.632143	71.300647
761.610729	40.603943	71.305652
760.913228	36.083703	71.310657
760.493822	38.569436	71.315662
759.524579	34.713746	71.320666
758.567085	40.226021	71.325671
758.179427	43.998168	71.330676
757.787217	37.385690	71.335681
757.352643	35.710868	71.340686
756.402793	59.291438	71.345690
755.993488	35.383268	71.350695
755.287173	33.152490	71.355700
754.166681	41.264185	71.360705
753.833301	40.582460	71.365710
753.303141	40.564390	71.370714
752.494597	36.478126	71.375719
751.494863	46.814506	71.380724
750.942946	45.213555	71.385729
750.574719	22.046313	71.390734
749.688124	54.776908	71.395738
749.133544	36.237504	71.400743
748.244724	41.494434	71.405748
747.542341	29.662975	71.410753
747.495328	48.120014	71.415758
746.515803	50.111469	71.420762
745.830589	43.138799	71.425767
745.425026	39.533988	71.430772
744.403275	35.169446	71.435777
743.555392	51.271968	71.440782
742.836289	43.828475	71.445786
742.649140	33.927095	71.450791
742.082711	44.494104	71.455796
741.187891	44.100445	71.460801
740.471723	32.230183	71.465806
739.860876	40.990847	71.470810
739.518685	27.794817	71.475815
738.584746	31.155633	71.480820
737.872510	40.501692	71.485825
737.513804	39.992727	71.490830
736.511794	31.730149	71.495834
735.461829	46.767329	71.500839
734.927906	30.343981	71.505844
734.489752	37.907106	71.510849
734.087218	48.277724	71.515854
733.591258	33.586054	71.520858
732.909691	28.593379	71.525863
732.101029	39.683051	71.530868
731.381162	49.534934	71.535873
730.340094	24.000682	71.540878
729.251815	52.731297	71.545882
729.218029	10.427408	71.550887
729.030235	52.132729	71.555892
727.839700	23.536314	71.560897
726.929217	45.784441	71.565902
726.999850	39.033633	71.570906
726.544194	27.490897	71.575911
725.672613	32.770316	71.580916
724.584304	36.920502	71.585921
724.387335	30.830438	71.590926
722.926909	29.880309	71.595930
722.351074	33.843258	71.600935
721.687139	39.244157	71.605940
720.972401	41.409500	71.610945
720.926442	33.598669	71.615950
720.178688	35.195282	71.620954
719.597216	30.438976	71.625959
719.026128	32.168305	71.630964
718.187196	41.116665	71.635969
717.408605	33.927074	71.640974
716.502303	25.264513	71.645978
716.062660	49.982774	71.650983
716.041061	41.053205	71.655988
714.965278	28.809719	71.660993
714.307937	41.551529	71.665998
713.587733	42.185014	71.671002
712.629933	37.546965	71.676007
711.919604	38.040114	71.681012
711.094834	40.407472	71.686017
711.088605	35.338821	71.691022
709.969140	37.513410	71.696026
709.297065	31.894784	71.701031
708.747878	31.354651	71.706036
708.081014	37.594920	71.711041
707.876288	27.253246	71.716046
706.875137	35.298649	71.721050
706.082016	37.884886	71.726055
705.670073	39.191508	71.731060
704.943975	37.720798	71.736065
704.249042	32.222502	71.741070
703.264197	47.686120	71.746074
703.081202	38.980936	71.751079
702.358461	47.250091	71.756084
700.807036	36.469990	71.761089
700.680051	34.216377	71.766094
700.355419	42.691793	71.771098
700.090944	42.692933	71.776103
698.863839	35.350839	71.781108
698.020067	37.016360	71.786113
698.007426	30.559500	71.791118
697.115468	42.313694	71.796122
696.295067	35.731559	71.801127
695.593171	39.618394	71.806132
695.238918	33.766254	71.811137
694.097608	38.391646	71.816142
693.359175	42.131343	71.821146
693.239392	28.975605	71.826151
692.731233	36.701259	71.831156
691.413549	21.110744	71.836161
690.812904	49.295386	71.841166
690.462156	31.983489	71.846170
689.867641	20.041851	71.851175
689.216184	40.091563	71.856180
687.764010	40.789559	71.861185
687.455746	33.148222	71.866190
686.960700	32.142179	71.871194
686.562512	31.204289	71.876199
685.744232	31.375603	71.881204
684.648641	28.539806	71.886209
684.445302	32.192729	71.891214
683.995007	37.424009	71.896218
683.101339	33.403362	71.901223
682.481615	39.967276	71.906228
681.741621	32.596520	71.911233
681.573081	37.814478	71.916238
680.270005	40.969173	71.921242
679.734461	31.042857	71.926247
679.103655	39.615905	71.931252
678.222565	36.324929	71.936257
677.559406	33.477051	71.941262
676.857048	40.680145	71.946266
676.319389	30.276372	71.951271
676.482220	40.473395	71.956276
675.277720	23.882469	71.961281
674.534833	45.629277	71.966286
674.187922	37.374380	71.971290
673.280715	36.695726	71.976295
672.623022	29.303987	71.981300
671.845821	30.279281	71.986305
671.308178	34.685568	71.991310
670.234163	37.581456	71.996314
669.863877	47.489646	72.001319
669.368998	37.692466	72.006324
668.295959	39.132739	72.011329
667.361484	36.652900	72.016334
666.866647	41.610591	72.021338
666.754034	33.665305	72.026343
666.342615	35.596294	72.031348
665.444364	36.229758	72.036353
664.709322	32.603312	72.041358
664.262069	44.427050	72.046362
663.144227	12.659064	72.051367
662.233538	51.909149	72.056372
661.687658	39.248588	72.061377
661.379761	50.879839	72.066382
660.956866	49.252058	72.071386
660.012823	30.508219	72.076391
659.104920	44.597168	72.081396
658.566495	49.031971	72.086401
658.408410	40.918889	72.091406
657.390745	42.470192	72.096410
656.477402	35.223236	72.101415
656.208969	45.053709	72.106420
655.285623	54.209489	72.111425
654.535727	28.767685	72.116430
654.052006	55.191266	72.121434
653.557782	42.025763	72.126439
652.604761	27.096261	72.131444
651.676343	42.740126	72.136449
651.428547	37.351990	72.141454
650.569955	34.785962	72.146458
650.306479	44.524187	72.151463
649.445383	44.530450	72.156468
648.678128	30.638915	72.161473
648.260836	47.718357	72.166478
647.156659	32.453392	72.171482
646.372078	34.965750	72.176487
646.097955	37.412596	72.181492
645.436151	43.853915	72.186497
644.886376	37.200323	72.191502
643.857858	49.184428	72.196506
643.283715	38.759662	72.201511
643.128786	29.592730	72.206516
642.057157	41.547425	72.211521
641.079639	40.425837	72.216526
640.561927	43.187426	72.221530
639.915294	31.616779	72.226535
639.799582	39.503868	72.231540
639.009785	45.052555	72.236545
638.374680	36.993360	72.241550
637.423356	46.790655	72.246554
636.908355	45.466115	72.251559
635.776747	32.439966	72.256564
635.165160	39.336890	72.261569
634.747776	25.785452	72.266574
634.370296	60.305168	72.271578
633.878929	30.589853	72.276583
633.118291	46.273237	72.281588
632.308383	37.953310	72.286593
631.893641	37.678778	72.291598
630.575645	56.770258	72.296602
630.190541	33.794960	72.301607
629.680019	39.292869	72.306612
629.036355	38.102354	72.311617
628.210086	28.711184	72.316622
627.524715	42.627513	72.321626
627.165277	41.207244	72.326631
626.555585	39.126691	72.331636
625.351894	41.726294	72.336641
625.130871	36.542048	72.341646
624.399382	37.733995	72.346650
624.091743	41.701562	72.351655
622.789122	35.145785	72.356660
622.531926	36.681655	72.361665
621.479532	33.306022	72.366670
620.670154	40.321175	72.371674
619.910378	38.780163	72.376679
620.041941	33.352124	72.381684
619.387336	36.479274	72.386689
618.123892	37.224523	72.391694
617.363594	40.195049	72.396698
616.891989	29.960542	72.401703
616.654107	30.613438	72.406708
615.504767	38.550011	72.411713
615.408418	30.693603	72.416718
614.270021	38.097025	72.421722
613.866286	44.658096	72.426727
612.800662	29.369671	72.431732
611.970120	43.868913	72.436737
611.787772	35.609901	72.441742
611.511358	31.770097	72.446746
610.414644	36.487765	72.451751
609.782666	31.296429	72.456756
608.807437	36.928264	72.461761
608.678288	30.687075	72.466766
607.760471	34.425396	72.471770
606.677719	35.297988	72.476775
606.774360	35.907074	72.481780
606.030378	33.983524	72.486785
605.376806	25.783791	72.491790
604.558991	29.698567	72.496794
603.950466	33.403404	72.501799
603.254527	28.993351	72.506804
602.028799	35.707397	72.511809
601.705712	23.702065	72.516814
601.360999	32.134948	72.521818
600.503780	25.509835	72.526823
599.760108	28.102419	72.531828
598.822544	26.094588	72.536833
598.588879	25.337085	72.541838
598.109768	31.509627	72.546842
596.899455	22.335745	72.551847
596.293387	21.137677	72.556852
595.773926	30.509823	72.561857
595.601380	27.161236	72.566862
594.679244	24.015598	72.571866
593.694117	31.247967	72.576871
593.413500	26.435902	72.581876
592.923559	29.317648	72.586881
591.785694	30.038180	72.591886
590.772275	35.784907	72.596890
590.533125	38.428029	72.601895
590.297720	30.466043	72.606900
588.953512	41.805028	72.611905
588.386081	25.270391	72.616910
587.978731	26.330305	72.621914
587.695573	29.084508	72.626919
587.043010	19.492241	72.631924
586.190705	35.150796	72.636929
585.837110	22.579498	72.641934
584.570508	33.521361	72.646938
583.767481	33.715509	72.651943
583.070865	32.956044	72.656948
582.614373	32.062148	72.661953
582.440366	26.022064	72.666958
581.340430	34.750257	72.671962
580.787695	23.120534	72.676967
580.414289	41.821893	72.681972
579.275874	32.442608	72.686977
578.736460	24.065440	72.691982
577.851470	36.315263	72.696986
577.119688	23.548742	72.701991
576.456456	31.433139	72.706996
575.522618	35.121985	72.712001
575.396552	25.493176	72.717006
575.041616	21.162861	72.722010
574.297404	38.347970	72.727015
573.513511	23.203931	72.732020
572.928227	16.562333	72.737025
572.426705	26.010466	72.742030
571.331685	29.877940	72.747034
570.578215	35.233207	72.752039
570.103590	18.734265	72.757044
569.725568	30.912806	72.762049
568.894552	30.505895	72.767054
567.992716	21.535201	72.772058
567.673878	24.175245	72.777063
566.907437	28.258459	72.782068
565.560668	43.831781	72.787073
565.577187	22.803084	72.792078
564.726497	32.521287	72.797082
564.214038	30.234464	72.802087
563.548431	31.952072	72.807092
562.724556	36.807646	72.812097
562.203463	36.521680	72.817102
561.757528	35.764873	72.822106
560.971564	41.128473	72.827111
560.303205	27.318999	72.832116
559.612369	35.244065	72.837121
559.051104	35.443869	72.842126
557.845938	33.801933	72.847130
557.301708	30.389550	72.852135
557.108004	23.430134	72.857140
556.425837	29.338568	72.862145
555.735052	26.122984	72.867150
554.918020	18.217377	72.872154
553.856926	38.690285	72.877159
553.888392	39.387017	72.882164
553.105260	24.507781	72.887169
551.788399	31.950686	72.892174
551.205719	42.461958	72.897178
550.850544	36.125891	72.902183
550.742649	21.187999	72.907188
549.525183	45.691091	72.912193
549.182411	26.733292	72.917198
548.441969	23.629694	72.922202
548.239711	35.813360	72.927207
547.288973	35.826051	72.932212
546.208825	48.285161	72.937217
545.797422	13.774516	72.942222
544.694825	56.566874	72.947226
544.111982	18.073518	72.952231
543.760397	40.836586	72.957236
543.335646	41.352103	72.962241
542.522668	24.955937	72.967246
541.748170	45.160870	72.972250
541.431665	36.967390	72.977255
540.321281	48.475729	72.982260
539.291973	43.144278	72.987265
539.080489	15.100112	72.992270
538.290556	40.235235	72.997274
538.012839	23.813742	73.002279
537.132530	26.910629	73.007284
536.198135	30.627961	73.012289
535.886106	35.389402	73.017294
535.078588	40.366953	73.022298
534.216338	35.849375	73.027303
533.734382	26.960044	73.032308
532.905335	47.323473	73.037313
532.742523	28.119405	73.042318
531.943708	33.494518	73.047322
530.936430	34.317275	73.052327
530.518991	45.999083	73.057332
530.034249	53.675307	73.062337
528.954972	29.285780	73.067342
528.179049	25.889810	73.072346
527.774545	51.256861	73.077351
527.778187	34.951385	73.082356
526.605149	29.420499	73.087361
526.181917	22.787792	73.092366
525.576123	26.589975	73.097370
524.664613	43.814357	73.102375
523.896028	33.034273	73.107380
523.159667	42.444136	73.112385
522.724366	31.934227	73.117390
521.497525	32.823497	73.122394
520.735706	48.787771	73.127399
520.541724	26.311919	73.132404
519.986268	36.443557	73.137409
519.864348	37.868007	73.142414
518.699873	34.254820	73.147418
518.051611	34.681368	73.152423
517.310750	43.563696	73.157428
516.300283	39.528604	73.162433
515.804118	26.391856	73.167438
514.978546	30.566500	73.172442
514.738786	38.034970	73.177447
514.533804	28.543311	73.182452
512.957829	26.231946	73.187457
512.629472	42.261205	73.192462
512.478471	45.863226	73.197466
511.133944	16.969843	73.202471
510.631365	44.383518	73.207476
509.804457	29.683150	73.212481
509.575407	23.402698	73.217486
508.939004	41.660267	73.222490
508.014031	37.559524	73.227495
507.486915	22.079742	73.232500
506.674852	40.362135	73.237505
505.951652	38.599302	73.242510
505.572356	17.247340	73.247514
504.844292	31.487426	73.252519
504.248371	35.261236	73.257524
503.339412	22.964495	73.262529
502.694062	36.339897	73.267534
502.166492	36.365621	73.272538
501.479116	37.036512	73.277543
500.685007	25.707025	73.282548
499.849182	36.933525	73.287553
499.552588	41.845470	73.292558
499.123807	21.575241	73.297562
497.849209	22.461092	73.302567
497.594058	23.725422	73.307572
496.810880	27.902780	73.312577
496.187718	29.884867	73.317582
495.218912	35.659211	73.322586
494.745358	35.200115	73.327591
494.327678	24.006202	73.332596
493.315592	27.617657	73.337601
492.613385	27.420478	73.342606
492.147764	38.364094	73.347610
491.568949	48.337046	73.352615
491.334455	38.033263	73.357620
490.281338	48.406606	73.362625
489.834287	36.154548	73.367630
488.947695	43.092152	73.372634
487.987159	47.502763	73.377639
487.587538	32.387426	73.382644
486.736818	41.665709	73.387649
486.629741	32.965819	73.392654
485.516937	31.580430	73.397658
484.675414	40.496143	73.402663
484.400801	29.400859	73.407668
483.742685	37.617182	73.412673
482.542871	44.912175	73.417678
482.041941	28.100493	73.422682
481.349026	32.392781	73.427687
481.275980	50.980070	73.432692
480.636369	36.109533	73.437697
479.618299	31.697221	73.442702
479.101145	29.630351	73.447706
478.345914	37.206164	73.452711
477.331077	42.704012	73.457716
476.367171	37.565592	73.462721
476.214225	25.698761	73.467726
475.750769	40.838102	73.472730
474.927376	45.781932	73.477735
474.793771	30.480729	73.482740
473.559286	31.300281	73.487745
473.092437	39.276413	73.492750
472.526326	36.283832	73.497754
471.600433	35.193511	73.502759
471.270662	22.719370	73.507764
470.604175	38.789872	73.512769
469.528124	18.875070	73.517774
468.884248	41.348819	73.522778
468.390717	31.882634	73.527783
468.330096	23.028702	73.532788
467.262298	25.127356	73.537793
466.173177	17.665657	73.542798
465.262102	29.911771	73.547802
465.001481	49.411987	73.552807
464.925408	25.789903	73.557812
463.461518	28.216573	73.562817
463.057600	39.432623	73.567822
462.928302	25.016948	73.572826
461.946198	27.901429	73.577831
461.505974	27.623101	73.582836
460.612640	31.510527	73.587841
459.600060	35.025885	73.592846
458.929076	44.449000	73.597850
458.159659	28.118471	73.602855
457.557705	40.116663	73.607860
457.311850	34.803940	73.612865
456.784280	27.711654	73.617870
455.903525	54.464956	73.622874
455.343621	38.484221	73.627879
454.890635	23.087261	73.632884
453.286199	32.946067	73.637889
452.500459	51.251094	73.642894
452.185739	19.740076	73.647898
451.825681	45.841160	73.652903
451.705013	22.062194	73.657908
450.898641	43.314525	73.662913
450.121975	44.196765	73.667918
449.712245	35.953505	73.672922
448.353344	34.738220	73.677927
447.889748	31.759274	73.682932
447.101441	29.369775	73.687937
447.042464	22.969203	73.692942
445.766183	25.927362	73.697946
444.921032	44.412149	73.702951
444.663481	28.529911	73.707956
444.092572	12.054247	73.712961
443.098703	45.292316	73.717966
442.676837	13.596545	73.722970
441.948991	48.957289	73.727975
442.021289	27.156520	73.732980
440.520513	32.895788	73.737985
440.298114	37.657150	73.742990
439.984036	13.841209	73.747994
438.531748	52.057982	73.752999
437.860462	20.226902	73.758004
436.950831	52.741973	73.763009
436.745592	10.577501	73.768014
435.589679	46.818527	73.773018
435.006934	6.466120	73.778023
434.758194	47.457237	73.783028
434.036115	18.728089	73.788033
433.524808	49.940271	73.793038
432.659982	30.622577	73.798042
432.023146	22.989494	73.803047
431.659402	51.059111	73.808052
430.590375	39.454914	73.813057
430.331601	-2.852367	73.818062
429.425912	49.626861	73.823066
428.946872	40.593592	73.828071
428.506015	16.810464	73.833076
427.219382	57.889696	73.838081
426.748324	21.999372	73.843086
426.351162	45.310563	73.848090
425.240266	51.648443	73.853095
424.719516	20.871971	73.858100
424.158018	45.682145	73.863105
423.605791	20.738829	73.868110
423.113073	37.388746	73.873114
421.478642	47.712805	73.878119
421.362292	3.892669	73.883124
420.795052	54.662276	73.888129
420.728293	21.899143	73.893134
419.834568	45.264217	73.898138
418.958935	23.986626	73.903143
418.748298	46.689388	73.908148
417.399614	24.317123	73.913153
416.770310	42.322842	73.918158
416.499706	17.984339	73.923162
415.477240	38.217742	73.928167
414.699660	42.029975	73.933172
414.333408	33.335119	73.938177
413.610413	24.635609	73.943182
412.886357	43.405442	73.948186
411.936049	25.761837	73.953191
411.759968	28.134736	73.958196
410.817681	20.512482	73.963201
410.228607	36.709419	73.968206
409.423905	13.944591	73.973210
408.603689	52.860140	73.978215
408.464277	16.918576	73.983220
407.869487	33.173187	73.988225
406.969023	29.940596	73.993230
406.383225	35.043695	73.998234
405.681970	43.949696	74.003239
405.279040	23.150283	74.008244
404.006401	49.515031	74.013249
403.408838	21.984983	74.018254
402.917198	34.649964	74.023258
402.703728	32.132623	74.028263
401.721047	34.102632	74.033268
400.883225	45.594393	74.038273
400.281902	48.407193	74.043278
400.342015	6.873799	74.048282
398.642917	60.201680	74.053287
398.330660	26.395923	74.058292
397.899607	50.704374	74.063297
397.179499	18.069012	74.068302
396.051248	52.303017	74.073306
395.359061	19.235870	74.078311
395.131686	52.578900	74.083316
394.588721	17.483771	74.088321
393.978396	52.444190	74.093326
393.125461	8.118552	74.098330
392.443252	47.363738	74.103335
392.480134	20.098447	74.108340
390.851574	36.869420	74.113345
390.600678	23.379840	74.118350
389.823789	42.367816	74.123354
388.791454	34.774105	74.128359
388.291391	19.657472	74.133364
388.038109	35.643218	74.138369
387.502281	16.862899	74.143374
386.646601	38.312309	74.148378
385.454520	19.207641	74.153383
385.204660	39.863547	74.158388
384.652389	21.394911	74.163393
383.971661	43.686887	74.168398
383.250323	15.495374	74.173402
382.284229	56.562953	74.178407
382.216363	3.359002	74.183412
380.706507	58.343978	74.188417
379.902230	26.594033	74.193422
380.073190	9.132911	74.198426
379.336890	59.036946	74.203431
378.513422	28.065880	74.208436
377.832198	14.228585	74.213441
377.343209	59.946041	74.218446
376.969160	29.989831	74.223450
376.269753	35.096846	74.228455
375.294232	43.748524	74.233460
374.600366	10.932401	74.238465
374.098511	46.619804	74.243470
372.903073	16.772427	74.248474
372.121719	46.373483	74.253479
372.248813	22.741134	74.258484
371.454229	19.464883	74.263489
370.747348	49.481411	74.268494
370.173497	33.031453	74.273498
369.429653	21.823322	74.278503
368.712656	32.718692	74.283508
367.704884	25.083237	74.288513
367.086964	21.267929	74.293518
366.764682	29.851780	74.298522
366.177070	35.508659	74.303527
365.672883	18.156685	74.308532
364.635280	36.063465	74.313537
363.938423	30.019994	74.318542
363.836779	23.093245	74.323546
362.560708	28.173884	74.328551
361.971825	22.247247	74.333556
361.348802	36.049593	74.338561
360.736144	34.152502	74.343566
359.834868	30.175775	74.348570
359.158131	24.455515	74.353575
358.561660	34.970579	74.358580
358.633941	35.294967	74.363585
357.471584	42.923069	74.368590
357.217679	30.399019	74.373594
356.342881	30.645675	74.378599
355.515165	35.870907	74.383604
354.188327	46.611166	74.388609
353.515485	39.956771	74.393614
353.402346	15.998460	74.398618
352.686070	45.623835	74.403623
352.693272	25.167497	74.408628
351.620178	40.388217	74.413633
351.020560	44.646750	74.418638
350.631670	11.449323	74.423642
349.013331	38.119872	74.428647
348.468955	18.998747	74.433652
348.215354	23.269941	74.438657
348.011762	26.842497	74.443662
346.943253	30.250120	74.448666
345.937269	33.695086	74.453671
345.726715	26.899227	74.458676
344.880458	24.627803	74.463681
344.254270	26.118422	74.468686
343.672106	15.056422	74.473690
342.933059	37.419181	74.478695
342.453533	23.450408	74.483700
341.415794	30.759046	74.488705
340.467412	25.749098	74.493710
340.339096	19.883109	74.498714
339.757474	9.257822	74.503719
338.974025	20.171662	74.508724
338.103890	28.303525	74.513729
337.557889	24.019471	74.518734
337.476917	16.567489	74.523738
336.261448	28.653991	74.528743
336.034949	21.430191	74.533748
335.671885	11.932231	74.538753
333.841402	36.678115	74.543758
333.331528	28.133896	74.548762
332.612448	26.480843	74.553767
332.625190	35.779248	74.558772
331.872032	36.545819	74.563777
331.049190	29.694578	74.568782
330.689589	18.661765	74.573786
329.371618	40.951215	74.578791
328.602265	1.068583	74.583796
327.916560	28.867765	74.588801
327.527218	35.839705	74.593806
327.524598	22.884559	74.598810
326.550064	24.429117	74.603815
325.882341	23.767620	74.608820
325.351199	26.577131	74.613825
324.516745	22.616579	74.618830
323.729925	20.316768	74.623834
322.378879	16.537886	74.628839
322.234572	20.164068	74.633844
322.101782	18.644657	74.638849
321.080181	32.502638	74.643854
320.398655	23.266726	74.648858
319.924334	15.071650	74.653863
319.447873	33.499261	74.658868
318.269122	35.726041	74.663873
317.662852	20.761970	74.668878
317.623495	16.715712	74.673882
316.559083	20.438066	74.678887
315.817828	35.298417	74.683892
315.138263	15.751022	74.688897
314.623725	25.456707	74.693902
314.234265	17.902509	74.698906
312.895010	34.545413	74.703911
312.289398	19.852464	74.708916
311.568087	27.905426	74.713921
311.493653	14.264757	74.718926
310.463362	43.872364	74.723930
309.443384	19.727437	74.728935
309.521613	4.846679	74.733940
308.532470	23.803813	74.738945
308.298887	12.624778	74.743950
307.474317	30.759374	74.748954
306.731796	32.850409	74.753959
305.933582	8.605508	74.758964
304.797672	42.064896	74.763969
304.242707	13.433779	74.768974
304.180565	40.226905	74.773978
303.217176	30.066138	74.778983
302.612549	26.250306	74.783988
301.467397	28.236783	74.788993
301.435760	10.041597	74.793998
300.955355	30.852486	74.799002
300.014057	24.162057	74.804007
299.254014	27.030130	74.809012
298.638211	27.874163	74.814017
298.114082	32.524351	74.819022
296.930426	17.866766	74.824026
296.512419	5.668511	74.829031
295.905949	42.828013	74.834036
295.488917	27.926821	74.839041
294.815926	15.802310	74.844046
294.327054	15.033474	74.849050
293.652643	45.664526	74.854055
293.193193	63.059764	74.859060
291.804927	36.188752	74.864065
291.259877	23.373673	74.869070
291.086087	15.137016	74.874074
289.355173	38.790052	74.879079
288.960187	20.040938	74.884084
288.704299	11.957709	74.889089
288.298434	45.366983	74.894094
288.079342	14.747518	74.899098
286.977335	43.808344	74.904103
286.146377	5.397314	74.909108
285.757730	49.632227	74.914113
284.259829	37.697516	74.919118
283.843189	-3.572164	74.924122
283.230402	28.482403	74.929127
282.905154	59.084641	74.934132
282.265779	30.566299	74.939137
281.472721	2.428879	74.944142
280.761399	39.881035	74.949146
280.041014	45.560670	74.954151
279.884495	-2.352842	74.959156
279.062001	31.351446	74.964161
278.015910	29.925561	74.969166
277.799234	14.122022	74.974170
276.358370	35.215298	74.979175
276.042897	17.820668	74.984180
275.446223	21.824863	74.989185
275.054327	34.127042	74.994190
274.836548	5.245107	74.999194
273.455702	59.674967	75.004199
273.215861	48.233571	75.009204
271.917410	36.886794	75.014209
271.167343	12.583774	75.019214
270.665578	42.551822	75.024218
270.028034	48.249795	75.029223
270.048981	14.354756	75.034228
269.109350	-3.135898	75.039233
268.126472	39.988962	75.044238
267.583509	41.381184	75.049242
266.989239	39.340846	75.054247
266.625437	21.413050	75.059252
265.647308	13.094873	75.064257
265.046105	33.871404	75.069262
264.468111	33.014282	75.074266
263.175399	16.792498	75.079271
263.146242	32.985347	75.084276
262.696618	19.661511	75.089281
261.665867	45.612435	75.094286
260.780671	2.309152	75.099290
259.739923	36.051390	75.104295
259.754003	2.721998	75.109300
259.433229	51.224137	75.114305
258.457237	33.598898	75.119310
257.910386	21.265067	75.124314
257.282680	31.827695	75.129319
256.769200	26.739004	75.134324
255.397476	6.138242	75.139329
254.770090	35.910266	75.144334
254.523209	3.213796	75.149338
253.483495	34.232612	75.154343
253.019711	20.278710	75.159348
252.515882	32.567191	75.164353
251.928902	25.733581	75.169358
251.604256	13.720714	75.174362
250.318785	24.842318	75.179367
249.994510	46.706923	75.184372
248.915703	17.725683	75.189377
247.807572	34.418499	75.194382
247.734047	19.459426	75.199386
247.023046	19.799855	75.204391
246.730761	35.017562	75.209396
246.019029	6.960229	75.214401
244.906697	54.648727	75.219406
244.713886	18.759898	75.224410
244.123796	26.528620	75.229415
243.135049	5.038968	75.234420
242.276819	29.284577	75.239425
241.620925	34.709522	75.244430
241.750031	-4.434765	75.249434
240.307520	33.269526	75.254439
239.437000	22.057989	75.259444
239.502977	-6.284117	75.264449
238.108020	9.820491	75.269454
238.091566	39.971356	75.274458
237.024769	13.847091	75.279463
236.608378	33.922418	75.284468
236.344524	7.324844	75.289473
235.202798	36.959667	75.294478
234.191328	10.654711	75.299482
234.113262	2.590460	75.304487
233.548941	42.703017	75.309492
232.671253	32.583813	75.314497
231.706718	5.281112	75.319502
231.612011	33.498579	75.324506
230.836828	14.407994	75.329511
229.748304	27.440919	75.334516
229.216892	11.570876	75.339521
228.369392	31.987717	75.344526
228.095135	28.557616	75.349530
227.423089	9.379640	75.354535
226.619740	17.018359	75.359540
225.801814	38.144817	75.364545
225.487181	9.830238	75.369550
224.689921	46.376786	75.374554
223.827370	20.789212	75.379559
223.193658	39.464234	75.384564
222.686962	19.383149	75.389569
222.152075	28.492878	75.394574
221.733825	14.569579	75.399578
220.356398	25.297444	75.404583
220.192607	35.251571	75.409588
219.676515	6.063990	75.414593
218.429860	42.444055	75.419598
217.757994	20.612163	75.424602
217.035449	20.246426	75.429607
217.015901	30.496084	75.434612
216.148903	28.937605	75.439617
215.062586	22.826968	75.444622
214.903077	29.989346	75.449626
214.385443	52.348378	75.454631
213.485402	39.410138	75.459636
212.905560	7.272930	75.464641
212.374443	-4.022637	75.469646
211.865567	12.457951	75.474650
210.625703	46.034846	75.479655
210.104080	22.827624	75.484660
209.732608	32.748626	75.489665
208.249309	43.032939	75.494670
208.057483	34.017030	75.499674
207.221679	39.374474	75.504679
206.828420	11.017244	75.509684
206.450304	51.916957	75.514689
205.684521	17.582825	75.519694
205.016484	37.993145	75.524698
204.247753	21.659486	75.529703
203.532732	27.216858	75.534708
202.661705	12.227244	75.539713
202.098577	32.288113	75.544718
201.861132	39.546494	75.549722
201.027641	18.103060	75.554727
200.295883	4.791120	75.559732
199.607841	43.261373	75.564737
198.797123	26.671067	75.569742
198.810841	-6.104743	75.574746
197.476971	54.539926	75.579751
196.682855	22.649730	75.584756
196.401230	42.774543	75.589761
194.999600	35.257145	75.594766
194.488467	30.671117	75.599770
193.928761	56.662090	75.604775
193.845106	15.310946	75.609780
193.592858	37.644994	75.614785
192.305236	34.439516	75.619790
192.043678	-4.096878	75.624794
191.358475	51.029406	75.629799
190.381559	28.202256	75.634804
189.310193	24.345751	75.639809
189.169587	5.373224	75.644814
188.816135	-8.232383	75.649818
187.568667	-2.143885	75.654823
186.435801	11.008065	75.659828
186.361355	51.588139	75.664833
185.464413	33.018409	75.669838
185.637966	7.585816	75.674842
184.298109	17.270122	75.679847
183.583241	62.091602	75.684852
183.474811	52.146228	75.689857
181.798177	47.299745	75.694862
181.883462	37.605759	75.699866
180.842726	31.692863	75.704871
180.481621	5.134472	75.709876
180.160110	40.267973	75.714881
178.809127	38.624245	75.719886
178.150494	24.094333	75.724890
178.233550	10.400201	75.729895
177.384149	-0.226484	75.734900
176.504983	24.421407	75.739905
175.539881	56.377657	75.744910
175.328112	14.972835	75.749914
174.308573	13.892830	75.754919
173.679650	52.705322	75.759924
173.286320	-1.195611	75.764929
172.600514	34.092139	75.769934
171.940733	12.747187	75.774938
171.279817	44.744799	75.779943
170.586642	13.784672	75.784948
170.322592	36.858571	75.789953
169.152715	15.366290	75.794958
168.567488	44.541854	75.799962
168.418868	26.687009	75.804967
166.883298	30.844064	75.809972
166.593480	24.147600	75.814977
165.967930	21.035275	75.819982
165.077915	43.798993	75.824986
163.901230	20.404509	75.829991
163.416253	42.734664	75.834996
163.005639	18.759182	75.840001
162.666826	32.240282	75.845006
162.719858	34.529361	75.850010
161.436589	16.584200	75.855015
160.568285	42.137090	75.860020
160.421064	7.431600	75.865025
159.108000	43.267204	75.870030
158.501011	31.747192	75.875034
157.651332	25.423824	75.880039
157.697773	16.805165	75.885044
156.711499	31.890668	75.890049
155.740263	20.515466	75.895054
155.643026	40.344383	75.900058
154.837234	10.562804	75.905063
153.860233	43.580580	75.910068
153.419983	20.317840	75.915073
152.688787	33.595008	75.920078
152.212453	28.145626	75.925082
150.877708	26.910890	75.930087
150.163919	22.436029	75.935092
149.883376	23.863703	75.940097
149.467541	25.068533	75.945102
149.255105	20.381285	75.950106
148.174159	34.005935	75.955111
147.671606	21.613045	75.960116
146.802965	19.550256	75.965121
145.320102	40.073145	75.970126
145.404010	22.602263	75.975130
144.598818	20.270752	75.980135
144.314721	38.159946	75.985140
143.627488	26.681121	75.990145
142.396547	30.493171	75.995150
142.156212	26.318123	76.000154
141.815214	28.442952	76.005159
140.861079	25.729933	76.010164
140.086613	28.491546	76.015169
139.408010	29.774539	76.020174
139.201466	21.098448	76.025178
137.915861	14.417264	76.030183
137.119294	19.975034	76.035188
136.965642	23.318874	76.040193
136.181464	38.373744	76.045198
135.721600	28.948025	76.050202
134.389117	30.683761	76.055207
134.023753	32.897627	76.060212
133.868270	25.504851	76.065217
132.822654	28.792219	76.070222
132.155154	23.138370	76.075226
131.637359	31.475874	76.080231
131.101448	30.405504	76.085236
130.494512	19.005348	76.090241
129.358257	23.287980	76.095246
129.148082	31.197989	76.100250
128.469948	29.396552	76.105255
127.636995	26.284191	76.110260
127.073307	32.924417	76.115265
126.277439	37.521771	76.120270
125.741840	29.869495	76.125274
124.968991	32.774350	76.130279
124.336304	29.719941	76.135284
123.564463	23.737396	76.140289
122.469710	26.657308	76.145294
122.158205	14.886795	76.150298
121.643640	22.075819	76.155303
120.849280	34.267138	76.160308
120.861385	28.514394	76.165313
119.460729	10.917553	76.170318
119.147856	31.944562	76.175322
118.557315	20.357301	76.180327
117.427587	12.451279	76.185332
116.899342	31.795418	76.190337
116.313060	32.197996	76.195342
116.077628	14.524169	76.200346
114.749482	21.046596	76.205351
114.128465	36.010799	76.210356
113.760076	26.923722	76.215361
113.129395	29.509460	76.220366
112.532112	28.179236	76.225370
111.384150	25.867699	76.230375
110.716781	33.692919	76.235380
110.769625	28.864033	76.240385
110.072669	28.699240	76.245390
109.045839	24.693754	76.250394
108.362273	28.825374	76.255399
107.763685	25.819147	76.260404
107.439780	25.520760	76.265409
106.200522	27.708399	76.270414
106.057159	31.484240	76.275418
105.308501	31.078547	76.280423
104.146720	32.602587	76.285428
103.601324	25.191567	76.290433
102.830084	28.312202	76.295438
102.680348	18.411294	76.300442
102.022530	19.203731	76.305447
101.158342	44.017998	76.310452
100.910136	22.402447	76.315457
99.703064	27.506896	76.320462
99.044154	29.975720	76.325466
98.248679	41.604285	76.330471
97.727426	38.185202	76.335476
97.471750	27.899079	76.340481
96.319549	26.067593	76.345486
95.765134	40.970724	76.350490
95.375318	25.122294	76.355495
94.837192	28.861738	76.360500
94.165846	24.414820	76.365505
92.880349	37.893920	76.370510
92.498537	36.953521	76.375514
92.200710	25.448894	76.380519
91.237933	41.290725	76.385524
90.690937	37.615565	76.390529
89.367243	42.694467	76.395534
89.627264	19.955573	76.400538
88.627589	27.863743	76.405543
87.750409	43.017029	76.410548
87.615741	23.824373	76.415553
87.002921	37.614083	76.420558
86.247774	26.324298	76.425562
85.576501	41.485747	76.430567
84.510359	13.817732	76.435572
83.740103	37.724505	76.440577
82.805262	21.157211	76.445582
82.534148	46.589658	76.450586
82.243452	15.719937	76.455591
81.476602	44.311052	76.460596
80.545397	27.172346	76.465601
80.074537	8.916368	76.470606
79.720511	49.446360	76.475610
78.685777	14.792530	76.480615
77.560679	44.606078	76.485620
77.586835	21.245344	76.490625
76.713407	18.541559	76.495630
76.480652	32.541881	76.500634
75.143282	24.170696	76.505639
74.505251	24.665109	76.510644
74.380966	31.519111	76.515649
73.456048	24.581759	76.520654
72.597250	43.966010	76.525658
72.369070	5.604096	76.530663
71.490437	43.999074	76.535668
70.669890	2.991027	76.540673
69.820356	45.206847	76.545678
69.542049	47.190810	76.550682
68.912804	27.045749	76.555687
68.046729	50.132081	76.560692
67.492238	10.065558	76.565697
66.273809	31.615414	76.570702
66.618171	8.736941	76.575706
65.855356	26.437539	76.580711
64.727083	29.298169	76.585716
64.706177	29.348841	76.590721
63.573976	19.755989	76.595726
62.460666	29.446805	76.600730
62.218606	30.565592	76.605735
61.669950	23.448403	76.610740
61.545024	22.695691	76.615745
59.669494	39.140373	76.620750
59.451004	21.746112	76.625754
58.510665	19.915552	76.630759
58.328566	41.938794	76.635764
57.457859	2.152949	76.640769
56.697304	49.663900	76.645774
56.497332	49.654823	76.650778
56.140044	14.172351	76.655783
54.895841	31.954454	76.660788
54.443735	21.035808	76.665793
53.576024	25.868551	76.670798
52.802234	21.018537	76.675802
52.236879	3.655962	76.680807
51.098387	46.734680	76.685812
50.863502	24.735417	76.690817
50.574367	-5.929499	76.695822
49.805805	32.897301	76.700826
49.098621	2.062506	76.705831
48.399968	38.120233	76.710836
47.583919	16.306699	76.715841
46.639246	0.299229	76.720846
46.089544	39.070644	76.725850
45.319103	25.529970	76.730855
45.294070	8.508556	76.735860
44.831994	20.115483	76.740865
44.033697	11.957962	76.745870
43.459193	42.894739	76.750874
41.925574	20.522312	76.755879
41.331257	-3.225099	76.760884
40.739945	29.866751	76.765889
40.227882	37.429112	76.770894
40.071487	-0.330815	76.775898
39.256813	43.382189	76.780903
37.918320	27.469036	76.785908
38.013142	4.422223	76.790913
37.136600	57.177426	76.795918
36.309176	29.381465	76.800922
35.750450	3.311951	76.805927
35.171270	-6.495211	76.810932
34.735680	37.469538	76.815937
33.453949	36.298948	76.820942
32.782600	13.919906	76.825946
32.426966	-3.091343	76.830951
31.841274	46.097871	76.835956
31.687628	0.508348	76.840961
30.280020	34.189257	76.845966
29.637108	26.451630	76.850970
29.573044	35.426377	76.855975
28.510871	18.407941	76.860980
27.989271	46.630382	76.865985
27.057093	14.361814	76.870990
26.873619	31.164249	76.875994
25.605911	23.594073	76.880999
25.190091	-4.089273	76.886004
24.839429	45.056145	76.891009
24.276841	17.549121	76.896014
23.622291	18.896114	76.901018
22.542087	25.588767	76.906023
21.671943	20.922857	76.911028
20.839765	34.854781	76.916033
20.057210	14.117656	76.921038
19.480707	35.960947	76.926042
19.340551	10.468035	76.931047
19.123985	51.646260	76.936052
18.093207	4.375336	76.941057
17.098002	56.665360	76.946062
16.629477	16.812211	76.951066
16.431950	42.652350	76.956071
15.056743	20.119072	76.961076
14.796092	16.395116	76.966081
13.670820	37.471268	76.971086
13.792945	4.949432	76.976090
12.620291	31.542703	76.981095
11.606394	50.838173	76.986100
11.827491	2.156568	76.991105
10.754420	-0.583152	76.996110
9.763184	40.863661	77.001114
9.280919	7.142028	77.006119
8.662164	43.973879	77.011124
8.224971	15.615858	77.016129
7.132279	24.237440	77.021134
6.304162	27.244177	77.026139
6.113322	17.196887	77.031143
5.735279	4.793663	77.036148
4.586377	39.694822	77.041153
3.719527	20.401362	77.046158