Mon Mar 08 18:48:25 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.222467	92.151780	0.000000
-1.698602	80.196233	0.005005
-2.348509	49.393315	0.010010
-3.357787	9.858359	0.015014
-7.414374	-12.541920	0.020019
-12.631130	-12.572270	0.025024
-17.966544	-11.577645	0.030029
-22.371561	-15.589731	0.035034
-26.304943	-16.487060	0.040038
-30.510149	-8.846482	0.045043
-33.987059	-14.209748	0.050048
-37.469194	-2.930005	0.055053
-41.275469	-6.864121	0.060058
-44.744627	-13.725047	0.065062
-48.773558	-8.619765	0.070067
-52.183730	-5.224740	0.075072
-56.285366	-1.192723	0.080077
-60.236568	-13.997171	0.085082
-63.780288	-21.147349	0.090086
-67.723974	-10.661207	0.095091
-71.065914	-11.810510	0.100096
-75.003496	-11.464526	0.105101
-78.897911	-4.010638	0.110106
-82.365658	-22.516827	0.115110
-86.411083	-10.267266	0.120115
-90.119812	-7.814821	0.125120
-94.115983	-13.437327	0.130125
-97.549922	-21.259366	0.135130
-101.174977	-17.623421	0.140134
-105.239604	-10.937073	0.145139
-108.908194	-24.360494	0.150144
-112.808874	-11.999957	0.155149
-116.612574	-17.711477	0.160154
-120.035875	-17.460095	0.165158
-124.491416	-4.623092	0.170163
-127.811434	-6.130608	0.175168
-131.896482	-16.258140	0.180173
-135.640338	-10.080216	0.185178
-139.242163	-11.842350	0.190182
-143.186520	-5.444773	0.195187
-146.398534	-13.024628	0.200192
-150.140146	-13.286924	0.205197
-154.049414	-4.414533	0.210202
-157.796021	-5.350915	0.215206
-161.680104	-7.332885	0.220211
-165.400764	-11.717251	0.225216
-169.095994	-11.589551	0.230221
-172.937936	-8.302065	0.235226
-176.807605	-9.384348	0.240230
-180.505677	-6.905083	0.245235
-184.344314	-22.811598	0.250240
-187.746382	-14.042182	0.255245
-191.815304	-6.530311	0.260250
-195.424919	-11.265068	0.265254
-199.156237	-4.150820	0.270259
-202.984252	-14.487970	0.275264
-207.003341	-5.818732	0.280269
-210.582981	-1.437712	0.285274
-214.068486	-7.266089	0.290278
-218.332643	-6.404154	0.295283
-221.700859	-14.506141	0.300288
-225.418005	-9.344688	0.305293
-229.568925	2.972401	0.310298
-233.015497	-9.637914	0.315302
-236.936021	-9.302274	0.320307
-240.864815	-23.193267	0.325312
-244.354944	-10.978484	0.330317
-248.340037	-2.891735	0.335322
-251.758892	-15.107495	0.340326
-255.788367	0.580487	0.345331
-259.519741	-9.164907	0.350336
-263.481919	-5.706709	0.355341
-267.039890	-6.073825	0.360346
-270.525747	-9.052682	0.365350
-274.473967	-4.194869	0.370355
-278.261094	-14.330273	0.375360
-281.898189	-5.581554	0.380365
-286.113180	-1.146310	0.385370
-289.466314	7.312685	0.390374
-293.540536	5.682960	0.395379
-296.896302	-7.280776	0.400384
-300.600797	-14.329237	0.405389
-304.595872	-9.287290	0.410394
-308.415312	-4.606091	0.415398
-312.410694	-3.626059	0.420403
-315.793187	-15.727682	0.425408
-319.705341	1.445985	0.430413
-323.460560	-1.169691	0.435418
-327.024900	-11.395771	0.440422
-331.182290	0.999776	0.445427
-334.585431	-9.655705	0.450432
-338.464903	-10.546938	0.455437
-342.434020	-14.910275	0.460442
-345.911376	-9.317024	0.465446
-349.827088	-9.833469	0.470451
-353.460386	-4.995851	0.475456
-357.348666	-7.579188	0.480461
-361.311041	-10.262645	0.485466
-364.556176	-14.452974	0.490470
-368.660416	-9.800323	0.495475
-372.516443	-12.847648	0.500480
-376.033026	-18.749655	0.505485
-379.928389	-5.894434	0.510490
-383.573416	-10.123382	0.515494
-387.683126	4.962641	0.520499
-390.987202	-10.420211	0.525504
-395.029079	-3.580916	0.530509
-398.619651	-8.952293	0.535514
-402.422151	-13.468281	0.540518
-406.385245	-9.278047	0.545523
-410.014158	-9.878035	0.550528
-413.983489	-11.778173	0.555533
-417.273399	0.095812	0.560538
-420.901534	-12.218722	0.565542
-425.132092	-7.845406	0.570547
-428.593675	-6.857390	0.575552
-432.369511	-7.629410	0.580557
-436.516413	-4.731176	0.585562
-439.765774	-8.182759	0.590566
-444.279672	-1.439881	0.595571
-447.619779	-7.682182	0.600576
-451.717541	-12.477345	0.605581
-455.233757	0.259099	0.610586
-458.782985	-15.071876	0.615590
-462.571458	-2.678272	0.620595
-466.125437	-15.389324	0.625600
-470.086709	-15.857296	0.630605
-474.131354	-5.926804	0.635610
-477.538080	-10.266199	0.640614
-481.543323	-4.681481	0.645619
-485.023405	-6.342693	0.650624
-488.881363	-6.032403	0.655629
-492.972467	-4.238895	0.660634
-496.492085	-7.847494	0.665638
-500.362733	-0.002539	0.670643
-504.002908	-6.373438	0.675648
-507.703522	-10.208559	0.680653
-511.604531	-7.164981	0.685658
-515.033818	-16.122463	0.690662
-519.039057	2.237960	0.695667
-522.729229	-10.648355	0.700672
-526.657664	-8.112848	0.705677
-530.340273	-7.688583	0.710682
-534.279439	-1.975571	0.715686
-538.363937	-4.317545	0.720691
-541.664216	-6.087814	0.725696
-545.466415	1.511327	0.730701
-549.455640	0.718389	0.735706
-552.791025	1.274868	0.740710
-556.560741	-0.753106	0.745715
-560.193815	-4.449134	0.750720
-563.839412	-2.450726	0.755725
-567.980759	-12.480170	0.760730
-571.575431	-14.025182	0.765734
-575.537987	-2.690054	0.770739
-579.072299	-13.543380	0.775744
-582.943144	-4.039423	0.780749
-586.991559	-12.278185	0.785754
-590.476815	-13.939990	0.790758
-594.338118	-7.376787	0.795763
-598.329728	-5.893867	0.800768
-601.928591	-5.889698	0.805773
-605.872349	-13.057119	0.810778
-609.492871	-15.318563	0.815782
-612.924108	-9.984603	0.820787
-616.456513	-13.600436	0.825792
-620.530774	-7.913010	0.830797
-624.689284	2.324482	0.835802
-628.126934	-18.626581	0.840806
-631.622438	-14.032908	0.845811
-635.702138	-16.455895	0.850816
-639.223329	-8.023211	0.855821
-643.265591	-9.431947	0.860826
-646.938776	-9.617671	0.865830
-651.078263	-7.363608	0.870835
-654.843949	-17.170656	0.875840
-658.365947	-14.032872	0.880845
-662.049711	-7.289789	0.885850
-665.374114	-16.445136	0.890854
-669.515800	-3.843415	0.895859
-673.242741	-5.627317	0.900864
-677.105849	-7.154503	0.905869
-681.163318	-3.212075	0.910874
-684.703339	-10.702480	0.915878
-688.540871	-8.966506	0.920883
-691.620884	-10.334974	0.925888
-695.536024	1.940451	0.930893
-699.617483	-0.792785	0.935898
-703.364300	-15.036864	0.940902
-707.403260	-2.479880	0.945907
-711.223839	-14.405230	0.950912
-714.747451	-16.202635	0.955917
-718.371094	-10.232272	0.960922
-721.711209	-17.730909	0.965926
-725.954338	-8.427419	0.970931
-729.790332	-9.559908	0.975936
-733.425763	-9.470853	0.980941
-737.282823	-3.955130	0.985946
-741.003243	-13.807113	0.990950
-744.972765	-10.726979	0.995955
-748.421441	-13.654295	1.000960
-752.231687	-3.981580	1.005965
-756.212946	-3.315280	1.010970
-759.891782	-18.010063	1.015974
-763.845173	-3.107707	1.020979
-767.460219	-10.466149	1.025984
-771.300368	-21.680255	1.030989
-775.014509	-7.817424	1.035994
-778.058963	-8.653758	1.040998
-782.383383	-14.742959	1.046003
-786.044156	-17.849190	1.051008
-789.874308	-18.965169	1.056013
-794.285770	-13.251940	1.061018
-797.355721	-13.759342	1.066022
-801.169903	-19.045456	1.071027
-804.772192	-19.724780	1.076032
-808.676344	-15.127029	1.081037
-812.356071	-22.484514	1.086042
-815.944726	-18.957403	1.091046
-820.405408	-0.664070	1.096051
-823.865174	-12.905504	1.101056
-827.733615	-13.983763	1.106061
-831.436037	-15.358197	1.111066
-834.783613	-19.187730	1.116070
-839.116037	-4.096944	1.121075
-842.567073	-12.940064	1.126080
-845.936319	-16.389252	1.131085
-849.561036	-11.605888	1.136090
-853.392547	-7.729256	1.141094
-857.775679	-8.663685	1.146099
-861.370958	-13.849087	1.151104
-865.362407	-8.346370	1.156109
-869.066631	-8.963571	1.161114
-872.365211	-13.622420	1.166118
-876.816832	-14.556901	1.171123
-880.258735	-10.078666	1.176128
-883.723225	-16.311468	1.181133
-887.781773	-0.650993	1.186138
-891.326391	-9.417580	1.191142
-895.411983	-8.444225	1.196147
-899.046137	-15.214387	1.201152
-902.875889	-15.366793	1.206157
-906.526283	-3.291065	1.211162
-909.967145	-5.244900	1.216166
-913.908935	-5.652168	1.221171
-917.904650	-16.729190	1.226176
-921.411667	-10.532765	1.231181
-925.834922	-5.525412	1.236186
-928.950115	-6.894248	1.241190
-932.565257	-8.112178	1.246195
-936.114454	-10.450745	1.251200
-939.944344	-11.109235	1.256205
-944.287589	-14.309495	1.261210
-947.937338	-13.561852	1.266214
-951.845710	-6.777689	1.271219
-955.924921	-6.390258	1.276224
-959.206626	-11.229863	1.281229
-963.002974	-12.937548	1.286234
-966.704693	-23.927458	1.291238
-970.930775	-10.884435	1.296243
-974.518171	-7.257946	1.301248
-977.810408	-6.354556	1.306253
-981.932667	-8.844240	1.311258
-985.283144	-11.914629	1.316262
-989.284910	-12.793115	1.321267
-992.748264	-14.946640	1.326272
-996.542039	-16.571109	1.331277
-1000.582420	-5.861496	1.336282
-1004.273090	-17.294630	1.341286
-1008.288550	-9.887745	1.346291
-1011.866237	-15.693842	1.351296
-1015.328785	-12.032072	1.356301
-1019.451860	-7.753753	1.361306
-1022.984606	-8.150572	1.366310
-1026.961610	-3.338977	1.371315
-1030.636257	-17.176159	1.376320
-1034.595728	-16.657943	1.381325
-1038.380778	-11.318833	1.386330
-1042.095784	-17.028806	1.391334
-1045.706813	-10.993749	1.396339
-1049.317130	-4.660776	1.401344
-1053.009024	-13.263203	1.406349
-1057.285670	-12.859783	1.411354
-1060.813007	-13.741498	1.416358
-1064.328337	2.612898	1.421363
-1068.421987	-16.986778	1.426368
-1071.596101	-23.429726	1.431373
-1075.859630	-5.440295	1.436378
-1079.462174	-10.777143	1.441382
-1083.569520	-6.435003	1.446387
-1087.201945	-11.159973	1.451392
-1091.080924	-8.245126	1.456397
-1094.902007	-12.599306	1.461402
-1098.032959	-15.307283	1.466406
-1101.932138	-1.948926	1.471411
-1106.050053	-9.653695	1.476416
-1109.561722	-17.584739	1.481421
-1113.201677	-14.611908	1.486426
-1116.914205	-19.467505	1.491430
-1120.996802	-2.109295	1.496435
-1124.612553	-8.550900	1.501440
-1128.506444	-3.156389	1.506445
-1132.368682	-1.767379	1.511450
-1135.890658	-11.186850	1.516454
-1139.621512	-9.129769	1.521459
-1143.434780	0.041013	1.526464
-1147.414815	-5.385130	1.531469
-1151.438822	-5.990138	1.536474
-1154.435793	-16.252035	1.541478
-1158.309389	-9.799513	1.546483
-1162.214168	-11.831695	1.551488
-1166.183146	-0.275436	1.556493
-1170.189104	-0.563201	1.561498
-1173.570339	-17.402080	1.566502
-1177.116274	-20.343145	1.571507
-1181.278266	-13.379275	1.576512
-1184.910468	-12.886364	1.581517
-1188.677577	-8.346192	1.586522
-1192.732727	-14.417773	1.591526
-1196.120958	-11.213878	1.596531
-1199.793609	-18.037307	1.601536
-1203.561754	-18.531789	1.606541
-1207.415995	-6.270061	1.611546
-1210.928637	-12.008984	1.616550
-1214.988051	-12.942504	1.621555
-1218.453948	-17.496804	1.626560
-1222.177383	-22.908681	1.631565
-1226.436239	-7.816404	1.636570
-1230.075111	-10.997964	1.641574
-1233.966108	-1.319476	1.646579
-1237.499632	-13.147919	1.651584
-1240.939342	-13.904621	1.656589
-1245.058052	-13.388946	1.661594
-1248.680425	-20.086307	1.666598
-1252.598883	-22.573427	1.671603
-1256.638788	-4.832362	1.676608
-1260.486935	-15.085609	1.681613
-1263.966134	-14.550835	1.686618
-1267.021444	-25.793482	1.691622
-1271.078575	-1.884207	1.696627
-1274.812000	-27.399065	1.701632
-1278.835046	-21.958416	1.706637
-1283.291722	-10.196198	1.711642
-1286.347977	-24.135058	1.716646
-1290.039279	-20.482006	1.721651
-1293.693676	-24.007879	1.726656
-1297.626597	-23.051952	1.731661
-1301.832322	-9.240560	1.736666
-1305.416657	-24.901920	1.741670
-1308.818960	-13.901315	1.746675
-1312.794763	-15.226486	1.751680
-1316.540077	-17.159359	1.756685
-1320.448967	-11.445195	1.761690
-1323.925631	-21.896549	1.766694
-1327.701001	-16.620032	1.771699
-1331.685785	-15.551674	1.776704
-1335.336503	-21.561585	1.781709
-1339.197720	-10.705078	1.786714
-1342.801745	-19.153933	1.791718
-1346.568306	-12.995768	1.796723
-1350.234033	-18.654773	1.801728
-1353.998840	-26.945411	1.806733
-1358.018560	-20.194812	1.811738
-1361.379990	-21.589868	1.816742
-1365.415619	-8.573518	1.821747
-1369.329837	-14.274707	1.826752
-1372.910117	-13.673128	1.831757
-1376.985449	-15.158860	1.836762
-1380.148128	-8.703110	1.841766
-1383.814905	-12.461807	1.846771
-1387.708635	-20.410077	1.851776
-1391.616769	-12.411086	1.856781
-1395.843713	-11.327499	1.861786
-1399.243754	-16.950118	1.866790
-1402.847529	-18.247970	1.871795
-1406.977733	-20.003961	1.876800
-1410.547345	-14.489041	1.881805
-1414.798409	-4.984415	1.886810
-1418.291467	-18.075769	1.891814
-1421.913084	-4.832323	1.896819
-1425.473030	-14.518032	1.901824
-1428.876938	-17.885113	1.906829
-1432.935447	-14.141504	1.911834
-1436.568195	-24.614985	1.916838
-1440.697408	-20.084242	1.921843
-1444.732107	2.751038	1.926848
-1448.133107	-19.975273	1.931853
-1452.463271	-7.487164	1.936858
-1455.771866	-15.888530	1.941862
-1459.354096	-26.691734	1.946867
-1463.143506	1.318877	1.951872
-1466.517367	-25.371172	1.956877
-1470.586130	-13.899377	1.961882
-1474.306488	-19.664536	1.966886
-1478.181170	-13.305938	1.971891
-1482.479024	-11.791400	1.976896
-1485.752860	-15.855687	1.981901
-1489.621294	-8.715960	1.986906
-1493.006009	-21.482363	1.991910
-1496.848803	-16.477034	1.996915
-1500.845401	-16.019720	2.006912
-1502.202396	-9.572208	2.016909
-1499.527695	-17.536372	2.026906
-1496.703604	-13.858324	2.036902
-1494.551556	-11.438354	2.046899
-1492.433706	-12.982139	2.056896
-1490.623173	-7.673433	2.066893
-1488.759160	-14.164158	2.076890
-1487.099078	-0.529748	2.086886
-1484.814503	-18.992366	2.096883
-1482.904940	-11.817523	2.106880
-1481.044413	-23.773664	2.116877
-1479.649360	-1.744684	2.126874
-1477.613676	-14.368316	2.136870
-1475.285018	-18.017296	2.146867
-1473.567408	-17.213951	2.156864
-1471.574049	-10.474069	2.166861
-1469.833900	-9.746956	2.176858
-1467.941110	-12.010949	2.186854
-1466.009034	-5.764900	2.196851
-1464.285867	-11.967806	2.206848
-1461.906588	-14.227596	2.216845
-1460.457765	-8.984095	2.226842
-1458.697901	-6.319720	2.236838
-1456.501026	-13.735249	2.246835
-1454.832109	-11.605750	2.256832
-1452.593412	-15.502393	2.266829
-1450.952158	-17.519264	2.276826
-1449.072925	-15.799206	2.286822
-1447.365100	-15.396880	2.296819
-1445.450023	-13.257846	2.306816
-1443.350038	-20.444701	2.316813
-1441.434094	-8.595859	2.326810
-1439.371547	-23.314158	2.336806
-1437.842954	-14.662044	2.346803
-1435.956187	-11.907452	2.356800
-1434.214863	-25.551214	2.366797
-1432.081599	-17.289583	2.376794
-1429.915183	-17.911143	2.386790
-1428.133839	-20.406717	2.396787
-1426.445508	-22.816348	2.406784
-1424.744673	-11.343552	2.416781
-1423.108672	-18.195589	2.426778
-1420.678302	-16.492703	2.436774
-1418.602678	-18.920133	2.446771
-1417.158191	-24.544729	2.456768
-1415.276086	-21.530444	2.466765
-1413.559276	-12.163227	2.476762
-1411.468042	-17.409824	2.486758
-1409.666032	-19.231365	2.496755
-1407.618318	-22.816351	2.506752
-1405.649726	-25.507667	2.516749
-1403.763956	-20.488816	2.526746
-1401.833128	-25.390792	2.536742
-1400.424691	-14.968465	2.546739
-1398.214490	-14.269190	2.556736
-1396.261651	-22.018201	2.566733
-1394.387602	-17.243765	2.576730
-1392.566949	-16.561060	2.586726
-1390.937431	-27.518631	2.596723
-1389.027096	-22.931570	2.606720
-1387.248623	-18.962830	2.616717
-1384.824642	-19.865570	2.626714
-1382.967731	-20.447008	2.636710
-1381.550892	-18.779173	2.646707
-1379.621616	-25.659185	2.656704
-1377.688391	-17.821762	2.666701
-1375.557163	-25.635628	2.676698
-1373.751985	-20.521748	2.686694
-1372.163959	-22.912125	2.696691
-1370.086272	-21.146409	2.706688
-1368.385231	-18.515176	2.716685
-1366.533347	-25.684350	2.726682
-1364.429704	-18.141023	2.736678
-1362.517098	-16.367817	2.746675
-1360.497301	-23.852798	2.756672
-1358.971936	-23.394357	2.766669
-1357.147045	-18.615178	2.776666
-1355.080468	-21.503707	2.786662
-1352.927610	-14.102448	2.796659
-1351.345237	-13.596289	2.806656
-1349.381186	-17.759903	2.816653
-1347.414990	-16.620489	2.826650
-1345.863002	-12.504938	2.836646
-1343.868672	-19.878470	2.846643
-1341.670130	-21.845536	2.856640
-1340.186688	-7.342778	2.866637
-1338.341443	-17.179137	2.876634
-1336.202192	-15.453241	2.886630
-1334.225249	-14.478158	2.896627
-1332.606227	-21.733184	2.906624
-1330.613907	-13.583088	2.916621
-1329.006906	-25.646955	2.926618
-1326.933208	-13.082777	2.936614
-1324.823273	-23.766708	2.946611
-1323.038576	-19.307889	2.956608
-1321.270376	-18.986183	2.966605
-1319.819954	-14.854356	2.976602
-1317.756729	-11.712671	2.986598
-1315.128139	-10.575052	2.996595
-1313.712209	-13.637278	3.006592
-1311.850675	-14.730948	3.016589
-1310.296783	-14.033897	3.026586
-1308.186605	-16.144674	3.036582
-1306.179872	-21.936569	3.046579
-1304.147713	-20.005618	3.056576
-1302.640271	-15.646079	3.066573
-1300.669368	-18.074011	3.076570
-1298.651560	-2.771008	3.086566
-1296.694281	-8.776024	3.096563
-1295.310867	-24.255464	3.106560
-1293.247687	-22.853649	3.116557
-1291.288780	-25.115451	3.126554
-1289.358960	-16.086944	3.136550
-1287.439619	-15.451528	3.146547
-1285.742496	-19.739726	3.156544
-1283.548099	-10.205694	3.166541
-1281.945469	-17.151769	3.176538
-1280.144141	-4.117650	3.186534
-1278.012962	-10.513621	3.196531
-1276.062143	-18.393264	3.206528
-1274.419926	-14.645767	3.216525
-1272.283429	-21.655175	3.226522
-1270.860914	-14.492184	3.236518
-1268.672763	-8.468510	3.246515
-1266.796800	-7.287743	3.256512
-1264.856796	-13.105242	3.266509
-1263.138219	-9.297328	3.276506
-1261.521978	-15.792438	3.286502
-1259.362064	-5.649736	3.296499
-1257.253507	-11.279481	3.306496
-1255.737189	-10.983724	3.316493
-1253.697899	-7.650264	3.326490
-1251.834257	-10.564646	3.336486
-1249.876662	-7.407570	3.346483
-1247.914696	-15.693165	3.356480
-1246.349234	-6.977331	3.366477
-1244.358206	0.388370	3.376474
-1242.360782	-7.970790	3.386470
-1240.606025	-6.203795	3.396467
-1238.483226	-8.600726	3.406464
-1236.825153	-12.304782	3.416461
-1234.776931	-5.000329	3.426458
-1233.298145	-9.455647	3.436454
-1231.147395	-11.437068	3.446451
-1229.203646	-5.052154	3.456448
-1227.342656	-10.686463	3.466445
-1225.482717	-9.820449	3.476442
-1223.853210	-5.256187	3.486438
-1221.790605	-3.603174	3.496435
-1220.158558	-10.111842	3.506432
-1217.854026	-2.657347	3.516429
-1216.276361	-8.202102	3.526426
-1214.159699	-9.183373	3.536422
-1212.517974	-1.005472	3.546419
-1210.500610	-5.949572	3.556416
-1208.672013	-9.526169	3.566413
-1207.065313	-2.919940	3.576410
-1204.841433	-11.594764	3.586406
-1203.108819	-15.620181	3.596403
-1200.826537	-6.821660	3.606400
-1199.262082	-10.273882	3.616397
-1197.746865	-14.529756	3.626394
-1195.715309	-6.542113	3.636390
-1193.723210	-12.944176	3.646387
-1191.527979	-11.920219	3.656384
-1189.662472	-15.024313	3.666381
-1188.113637	-12.846980	3.676378
-1186.149996	-10.017640	3.686374
-1184.552909	-6.654409	3.696371
-1182.310411	-12.504458	3.706368
-1180.225143	-3.980687	3.716365
-1178.881253	-2.637347	3.726362
-1176.964960	-4.514892	3.736358
-1174.529888	-8.644795	3.746355
-1172.842725	-12.530295	3.756352
-1171.434353	0.765742	3.766349
-1169.494276	-0.463535	3.776346
-1167.086521	-6.794726	3.786342
-1165.534774	-7.384002	3.796339
-1163.581094	-10.827430	3.806336
-1161.750952	-1.089727	3.816333
-1159.808375	-4.659264	3.826330
-1158.106520	-8.594471	3.836326
-1156.112519	-9.660268	3.846323
-1154.348169	-1.096175	3.856320
-1152.314468	-8.663746	3.866317
-1150.388216	-11.619644	3.876314
-1148.673839	-6.334736	3.886310
-1146.782910	-11.676950	3.896307
-1144.983800	-8.104448	3.906304
-1143.146441	-8.884661	3.916301
-1141.078048	-11.525417	3.926298
-1139.031655	-13.649523	3.936294
-1137.228610	-9.780819	3.946291
-1135.381836	-13.694987	3.956288
-1133.778093	-14.553072	3.966285
-1131.641639	-10.515087	3.976282
-1129.827630	-13.356700	3.986278
-1128.101032	-15.199120	3.996275
-1126.036950	-9.711210	4.006272
-1124.159063	-10.598939	4.016269
-1122.155538	-9.440041	4.026266
-1120.667428	-1.635364	4.036262
-1118.774269	-6.057440	4.046259
-1116.572470	-5.666006	4.056256
-1114.863159	-10.259181	4.066253
-1113.003023	-15.651702	4.076250
-1111.241045	-3.777907	4.086246
-1108.989453	-22.617034	4.096243
-1107.322590	1.951797	4.106240
-1105.517256	-0.601060	4.116237
-1103.557636	-15.264765	4.126234
-1101.821002	-1.318600	4.136230
-1099.969349	-8.174939	4.146227
-1097.682704	-9.188035	4.156224
-1096.153733	-22.661843	4.166221
-1094.456483	-4.902748	4.176218
-1092.395990	-8.958437	4.186214
-1090.214520	-13.589234	4.196211
-1088.263314	-13.923431	4.206208
-1086.794893	-15.857144	4.216205
-1084.819360	-11.561279	4.226202
-1083.161145	-9.928710	4.236198
-1080.843281	-10.277347	4.246195
-1079.061566	-4.472658	4.256192
-1077.245386	-16.748265	4.266189
-1075.475619	-14.686718	4.276186
-1073.628853	-12.326451	4.286182
-1071.774677	-4.100324	4.296179
-1069.966786	-17.053510	4.306176
-1067.835647	-5.731334	4.316173
-1066.116204	0.916968	4.326170
-1064.230044	-8.695241	4.336166
-1062.265194	-12.029854	4.346163
-1060.533738	-8.847491	4.356160
-1058.350083	-15.943209	4.366157
-1056.610054	-12.269612	4.376154
-1054.938978	-5.190433	4.386150
-1052.865535	-18.129245	4.396147
-1050.766690	-8.595471	4.406144
-1049.393645	-7.880367	4.416141
-1047.094543	-9.302752	4.426138
-1045.452936	-6.109164	4.436134
-1043.734002	-11.619568	4.446131
-1041.714508	-11.978859	4.456128
-1039.628354	-17.042761	4.466125
-1038.103565	-7.265583	4.476122
-1035.798936	-8.218341	4.486118
-1034.048741	-3.629031	4.496115
-1032.266041	-15.357706	4.506112
-1030.455290	-18.375555	4.516109
-1028.482546	-7.277465	4.526106
-1026.526665	-10.789026	4.536102
-1024.899510	-2.344977	4.546099
-1022.846276	-9.498750	4.556096
-1020.861745	-9.983477	4.566093
-1019.266317	-17.935552	4.576090
-1017.416702	-11.315931	4.586086
-1015.589510	-13.329087	4.596083
-1013.294463	-16.192290	4.606080
-1011.662129	-12.894568	4.616077
-1009.460830	-12.525056	4.626074
-1007.880741	-17.733770	4.636070
-1006.305835	-15.058404	4.646067
-1004.088278	-24.554625	4.656064
-1002.260506	-12.527061	4.666061
-1000.295273	-19.835675	4.676058
-998.391821	-13.925663	4.686054
-996.690930	-17.928494	4.696051
-994.890004	-21.121577	4.706048
-993.051576	-16.502142	4.716045
-990.900713	-9.906993	4.726042
-989.085694	-12.387104	4.736038
-987.350546	-10.818871	4.746035
-985.127664	-7.154547	4.756032
-983.484770	-8.328249	4.766029
-981.713101	-14.439117	4.776026
-979.789983	-14.735576	4.786022
-977.817010	-5.203701	4.796019
-975.885577	-14.351004	4.806016
-973.862143	-14.137741	4.816013
-972.335601	-16.764326	4.826010
-970.562449	-11.474467	4.836006
-968.412733	-9.865155	4.846003
-966.646694	-10.780659	4.856000
-964.870792	-20.506204	4.865997
-963.005169	-10.096672	4.875994
-960.825143	-13.986638	4.885990
-958.805088	-13.160222	4.895987
-956.892649	-19.904602	4.905984
-955.407195	-19.700023	4.915981
-953.663479	-14.553858	4.925978
-951.705912	-1.776511	4.935974
-949.688481	-16.256734	4.945971
-947.994721	-25.519153	4.955968
-945.641667	-13.195031	4.965965
-944.037059	-18.972858	4.975962
-942.482015	-14.243331	4.985958
-940.534035	-15.934711	4.995955
-938.266465	-15.312059	5.005952
-936.613106	-22.873894	5.015949
-934.729603	-14.527612	5.025946
-932.859655	-20.960458	5.035942
-930.846741	-19.603959	5.045939
-929.192791	-15.717561	5.055936
-927.325331	-23.133636	5.065933
-925.193219	-10.796263	5.075930
-923.547906	-22.978133	5.085926
-921.546722	-26.790519	5.095923
-919.785492	-21.855539	5.105920
-917.963746	-19.549564	5.115917
-915.822880	-20.234453	5.125914
-914.374266	-14.690563	5.135910
-911.919442	-21.450586	5.145907
-910.207307	-10.217559	5.155904
-908.404672	-14.113448	5.165901
-906.546331	-23.099018	5.175898
-904.652054	-18.191613	5.185894
-903.063160	-16.440467	5.195891
-900.842697	-21.472045	5.205888
-898.733777	-11.120302	5.215885
-896.897995	-19.859115	5.225882
-895.239484	-14.885585	5.235878
-893.486173	-15.685322	5.245875
-891.691146	-17.446938	5.255872
-889.711614	-12.077912	5.265869
-887.840194	-13.625963	5.275866
-886.063123	-13.674796	5.285862
-884.150529	-16.533567	5.295859
-882.075855	-19.735601	5.305856
-880.347525	-21.442336	5.315853
-878.231003	-19.642907	5.325850
-876.475009	-18.047926	5.335846
-874.652992	-9.098103	5.345843
-872.646757	-10.842950	5.355840
-870.769925	-16.544262	5.365837
-868.877860	-11.124919	5.375834
-867.347085	-13.344769	5.385830
-865.439051	-12.522467	5.395827
-863.463541	-17.511693	5.405824
-861.665348	-13.657779	5.415821
-859.574702	-13.657256	5.425818
-857.607432	-7.241032	5.435814
-856.013405	-11.143004	5.445811
-853.980424	-16.356137	5.455808
-852.136977	-14.975633	5.465805
-850.231608	-8.544769	5.475802
-848.503056	-8.702654	5.485798
-846.387261	-13.527989	5.495795
-844.619309	-11.072834	5.505792
-842.593184	-17.821095	5.515789
-840.739284	-19.824178	5.525786
-839.226240	-12.962713	5.535782
-837.330753	-13.226219	5.545779
-835.392267	-21.242500	5.555776
-833.378621	-19.841824	5.565773
-831.438372	-13.351789	5.575770
-829.623598	-15.620174	5.585766
-827.804120	-15.213135	5.595763
-825.688687	-18.963187	5.605760
-823.929390	-5.393011	5.615757
-821.926948	-17.246675	5.625754
-820.444274	-11.624485	5.635750
-818.322961	-8.229533	5.645747
-816.411972	-16.857164	5.655744
-814.781652	-16.372512	5.665741
-812.694259	-12.700569	5.675738
-810.911474	-16.133764	5.685734
-808.996066	-9.316069	5.695731
-807.075823	-17.103637	5.705728
-805.230672	-13.601376	5.715725
-803.535490	-14.745419	5.725722
-801.512832	-11.576249	5.735718
-799.580118	-12.453538	5.745715
-797.669972	-9.608993	5.755712
-795.807993	-14.303718	5.765709
-793.715949	-17.200576	5.775706
-792.240703	-12.025576	5.785702
-790.270237	-16.173983	5.795699
-788.181042	-6.070011	5.805696
-786.609857	-13.094440	5.815693
-784.862743	-10.751166	5.825690
-782.735725	-6.543977	5.835686
-780.691410	-16.148107	5.845683
-779.048274	-7.521694	5.855680
-776.942584	-11.139103	5.865677
-775.099146	-11.695803	5.875674
-773.384244	-9.140539	5.885670
-771.347546	-10.637552	5.895667
-769.720089	-18.360928	5.905664
-767.673879	-21.970398	5.915661
-765.639786	-14.497462	5.925658
-764.176680	-14.846529	5.935654
-762.011403	-16.796694	5.945651
-760.287899	-19.677248	5.955648
-758.566083	-17.522532	5.965645
-756.366982	-5.858809	5.975642
-754.602252	-11.253187	5.985638
-752.435408	-11.664201	5.995635
-750.953374	-11.154225	6.005632
-748.938524	-19.296327	6.015629
-746.941614	-11.198514	6.025626
-745.114376	-10.967905	6.035622
-743.038051	-24.186403	6.045619
-741.509332	-0.210892	6.055616
-739.858467	-20.837323	6.065613
-737.668977	-3.884424	6.075610
-735.642272	-11.347923	6.085606
-733.820015	-22.863265	6.095603
-732.180742	-5.012468	6.105600
-730.202509	-17.064292	6.115597
-728.279299	-16.539551	6.125594
-726.583794	-23.932738	6.135590
-724.523127	-20.295916	6.145587
-722.616614	-19.991122	6.155584
-720.881912	-14.595449	6.165581
-719.141279	-18.151308	6.175578
-716.922882	-15.133338	6.185574
-714.887034	-12.739843	6.195571
-713.250236	-16.414887	6.205568
-711.514370	-19.916297	6.215565
-709.356864	-22.157262	6.225562
-707.928688	-22.341247	6.235558
-705.936581	-14.531563	6.245555
-703.726760	-7.940813	6.255552
-702.236765	-13.739649	6.265549
-700.140652	-8.232773	6.275546
-698.296140	-12.379927	6.285542
-696.289464	-17.861873	6.295539
-694.645980	-21.528498	6.305536
-692.875645	-10.898241	6.315533
-690.571214	-19.031314	6.325530
-688.705697	-8.367316	6.335526
-687.031355	-17.100715	6.345523
-685.185114	-22.356496	6.355520
-683.066598	-18.599414	6.365517
-681.550299	-21.121555	6.375514
-679.812213	-17.553137	6.385510
-677.795316	-16.084954	6.395507
-675.723990	-22.502428	6.405504
-673.713226	-14.086252	6.415501
-671.798359	-11.836010	6.425498
-670.261227	-12.727347	6.435494
-668.363573	-13.643136	6.445491
-666.337358	-10.130220	6.455488
-664.385373	-11.405196	6.465485
-662.726792	-14.101633	6.475482
-660.786552	-8.495607	6.485478
-658.922237	-14.894202	6.495475
-656.989029	-14.430997	6.505472
-655.305005	-7.871440	6.515469
-653.273685	-11.775267	6.525466
-651.460604	-10.037663	6.535462
-649.353353	-4.242006	6.545459
-647.430694	-10.793594	6.555456
-645.633489	-14.206871	6.565453
-643.764448	-10.318313	6.575450
-642.238758	-23.911364	6.585446
-640.184516	-17.008343	6.595443
-638.461591	-15.273692	6.605440
-636.090644	-18.800738	6.615437
-634.287454	-20.037705	6.625434
-632.457957	-17.093299	6.635430
-630.829212	-19.173925	6.645427
-628.974588	-22.444791	6.655424
-627.058076	-22.883585	6.665421
-625.042854	-18.824169	6.675418
-622.971906	-19.696561	6.685414
-621.479233	-17.113572	6.695411
-619.827064	-23.912429	6.705408
-617.220907	-11.680473	6.715405
-615.447320	-16.553565	6.725402
-613.832805	-10.189703	6.735398
-612.333248	-8.094097	6.745395
-610.160259	-19.008590	6.755392
-608.193713	-12.917273	6.765389
-606.129683	-17.562038	6.775386
-604.601138	-9.125590	6.785382
-602.699216	-18.684730	6.795379
-600.684760	-16.545072	6.805376
-598.814951	-15.260152	6.815373
-596.787586	-16.692372	6.825370
-595.148853	-9.983435	6.835366
-593.335299	-12.590906	6.845363
-591.192185	-16.874102	6.855360
-589.413589	-11.668484	6.865357
-587.677614	-17.654965	6.875354
-585.677101	-12.369540	6.885350
-583.687748	-13.358329	6.895347
-581.862786	-13.439847	6.905344
-580.052176	-17.414137	6.915341
-578.238935	-5.770682	6.925338
-576.465611	-13.089373	6.935334
-574.444203	-8.623549	6.945331
-572.641724	-3.786449	6.955328
-570.648068	-8.539939	6.965325
-568.858139	-9.062669	6.975322
-567.012552	7.620126	6.985318
-565.051062	-9.407093	6.995315
-563.181346	-9.631528	7.005312
-561.560400	5.119885	7.015309
-559.298655	-10.548519	7.025306
-557.396368	-3.736397	7.035302
-555.674656	-13.134095	7.045299
-553.970055	-6.355125	7.055296
-551.725818	1.038665	7.065293
-550.151508	-12.394758	7.075290
-548.493266	-8.646122	7.085286
-546.432786	-7.664762	7.095283
-544.203553	-6.691411	7.105280
-542.552918	-12.092681	7.115277
-540.504891	-11.668247	7.125274
-538.879049	-7.563919	7.135270
-537.085396	-2.043307	7.145267
-535.100863	-9.255191	7.155264
-532.967103	0.898761	7.165261
-531.318480	-2.455968	7.175258
-529.386937	-8.754691	7.185254
-527.328143	-12.089674	7.195251
-525.563560	-2.645656	7.205248
-523.687558	-2.950007	7.215245
-522.237746	-14.394677	7.225242
-520.021453	-1.735600	7.235238
-518.187981	-7.208690	7.245235
-516.331898	-6.530955	7.255232
-514.471785	-9.469474	7.265229
-512.654324	-4.020538	7.275226
-510.687054	-7.745080	7.285222
-508.690327	-7.118223	7.295219
-506.688123	-3.729216	7.305216
-505.013150	-9.789581	7.315213
-503.120786	-16.074130	7.325210
-501.392853	-12.988665	7.335206
-499.318256	-16.335621	7.345203
-497.412302	-3.930097	7.355200
-495.701870	-14.587473	7.365197
-493.950483	-11.401542	7.375194
-491.800530	-10.050760	7.385190
-489.981407	-17.641957	7.395187
-488.281478	-14.683056	7.405184
-486.012240	-17.715316	7.415181
-484.310260	-21.454302	7.425178
-482.708577	-15.145134	7.435174
-480.707821	-7.720283	7.445171
-478.467450	-15.757681	7.455168
-476.700386	-13.938384	7.465165
-475.271512	-9.985702	7.475162
-473.096453	-10.707232	7.485158
-471.054924	-13.429967	7.495155
-469.566120	-8.397431	7.505152
-467.542365	-13.477736	7.515149
-465.644234	-15.419707	7.525146
-463.650616	-18.804224	7.535142
-461.758652	-21.106767	7.545139
-460.152672	-13.533593	7.555136
-458.126831	-17.875311	7.565133
-456.286730	-18.582803	7.575130
-454.375406	-19.454819	7.585126
-452.376417	-13.573797	7.595123
-450.564985	-24.574095	7.605120
-448.653553	-18.135958	7.615117
-446.710310	-20.681930	7.625114
-445.064730	-17.738001	7.635110
-443.208720	-19.006944	7.645107
-441.389299	-23.555670	7.655104
-439.171522	-12.230898	7.665101
-437.533365	-24.823437	7.675098
-435.615274	-18.384773	7.685094
-433.850886	-21.404254	7.695091
-431.592040	-19.466100	7.705088
-430.010146	-21.341753	7.715085
-428.210420	-23.921631	7.725082
-425.958090	-19.304668	7.735078
-424.332973	-27.799526	7.745075
-422.418616	-19.075630	7.755072
-420.615497	-20.512943	7.765069
-418.429777	-17.611040	7.775066
-416.780854	-9.384721	7.785062
-415.269245	-17.130436	7.795059
-413.284080	-12.638156	7.805056
-411.040673	-18.591870	7.815053
-409.224122	-21.769656	7.825050
-407.372818	-15.121363	7.835046
-405.507258	-10.439458	7.845043
-403.961841	-16.556434	7.855040
-401.712014	-11.173292	7.865037
-399.975351	-14.335158	7.875034
-398.118318	-3.917422	7.885030
-396.231090	-9.820568	7.895027
-394.153448	-9.070752	7.905024
-392.291102	-7.800264	7.915021
-390.586683	-10.895399	7.925018
-388.821284	-10.833054	7.935014
-386.929944	-5.613696	7.945011
-384.878551	0.844787	7.955008
-383.062581	-8.239452	7.965005
-381.228653	-20.001160	7.975002
-379.255869	-2.070672	7.984998
-377.443598	-5.430904	7.994995
-375.350058	-16.059383	8.004992
-373.632880	-12.427393	8.014989
-372.180657	-7.808929	8.024986
-370.001773	-4.318546	8.034982
-367.993022	-10.001085	8.044979
-365.659635	-5.332266	8.054976
-364.254287	-9.167490	8.064973
-362.671152	-9.213386	8.074970
-360.605227	-11.933610	8.084966
-358.625411	-15.199004	8.094963
-356.978098	-11.936355	8.104960
-355.012225	-8.689829	8.114957
-352.848329	-7.772178	8.124954
-351.090974	-8.207445	8.134950
-349.380969	-4.237989	8.144947
-347.609947	-0.808774	8.154944
-345.154843	-9.720306	8.164941
-343.511199	-5.536577	8.174938
-341.938338	-8.002810	8.184934
-339.743626	2.912097	8.194931
-338.163748	-7.665928	8.204928
-336.136431	-12.546181	8.214925
-334.319973	-4.176023	8.224922
-332.417908	-1.735568	8.234918
-330.497104	-5.589913	8.244915
-328.663422	-3.593253	8.254912
-326.755863	-13.023638	8.264909
-324.721895	-5.656047	8.274906
-322.976029	-5.252656	8.284902
-321.335704	-11.537889	8.294899
-319.427910	-7.682089	8.304896
-317.409362	-11.083102	8.314893
-315.419888	-2.240046	8.324890
-313.403784	-12.868749	8.334886
-311.554662	-8.163615	8.344883
-310.038792	-16.813069	8.354880
-308.410075	-15.063134	8.364877
-306.149384	-11.341026	8.374874
-303.950963	-6.341138	8.384870
-302.268669	-12.124661	8.394867
-300.800719	-1.924185	8.404864
-298.703204	-9.333920	8.414861
-296.615575	-15.193197	8.424858
-294.889635	-14.658716	8.434854
-292.981688	-0.636550	8.444851
-290.995132	-8.857475	8.454848
-289.093652	-3.331771	8.464845
-287.519981	-1.113580	8.474842
-285.558537	-6.701667	8.484838
-283.420893	-1.000509	8.494835
-282.170218	-11.794359	8.504832
-279.863852	-7.940574	8.514829
-277.812642	-10.860476	8.524826
-276.103285	-14.234204	8.534822
-274.277630	-6.250710	8.544819
-272.357308	-6.835085	8.554816
-270.412861	-13.285668	8.564813
-268.792690	-11.308562	8.574810
-266.519149	-12.516131	8.584807
-264.826638	-6.072881	8.594803
-262.715566	-4.943041	8.604800
-261.212683	-10.208449	8.614797
-259.226102	-11.597564	8.624794
-257.251424	-10.840666	8.634791
-255.804020	0.626224	8.644787
-253.783004	-11.130539	8.654784
-251.727740	4.953851	8.664781
-249.602070	-9.579489	8.674778
-248.018492	-5.703456	8.684775
-246.168512	-4.547715	8.694771
-244.237704	-9.350916	8.704768
-242.453539	-8.925159	8.714765
-240.415623	-10.417185	8.724762
-238.286774	-0.060057	8.734759
-236.490537	-5.539637	8.744755
-235.086210	-9.369892	8.754752
-233.076316	-6.236073	8.764749
-230.774649	-8.641727	8.774746
-229.284012	-9.503260	8.784743
-227.340377	-2.703764	8.794739
-225.738885	-14.519854	8.804736
-223.513487	-6.619065	8.814733
-221.376559	-14.210283	8.824730
-219.762734	-9.039645	8.834727
-217.965332	-7.311832	8.844723
-216.012399	-14.341597	8.854720
-214.326505	-10.353983	8.864717
-212.311216	-8.773041	8.874714
-210.503979	-13.202825	8.884711
-208.553595	-7.616968	8.894707
-206.597566	-6.860210	8.904704
-204.686592	-11.372859	8.914701
-202.705670	-4.094579	8.924698
-200.962932	-18.517814	8.934695
-199.163947	-15.111897	8.944691
-197.094977	-16.015186	8.954688
-195.618957	-13.762403	8.964685
-193.721650	-21.852170	8.974682
-191.758928	-14.951489	8.984679
-189.574625	-23.617556	8.994675
-188.138933	-12.871883	9.004672
-186.089123	-16.366196	9.014669
-183.926226	-24.345189	9.024666
-182.237529	-11.702609	9.034663
-180.292789	-21.448282	9.044659
-178.656153	-14.487655	9.054656
-176.795749	-27.619180	9.064653
-174.644905	-30.592788	9.074650
-172.928982	-14.858377	9.084647
-171.270523	-27.327700	9.094643
-169.365085	-9.169953	9.104640
-167.218130	-18.332128	9.114637
-165.340626	-19.094313	9.124634
-163.879442	-23.254111	9.134631
-161.617768	-17.173181	9.144627
-159.608459	-16.325418	9.154624
-158.009464	-18.183102	9.164621
-156.049895	-13.040752	9.174618
-154.026928	-16.807058	9.184615
-152.189098	-11.149510	9.194611
-150.437377	-19.752833	9.204608
-148.563728	-15.533040	9.214605
-146.673102	-24.725340	9.224602
-144.903336	-13.935056	9.234599
-142.901947	-16.643221	9.244595
-141.053021	-12.833141	9.254592
-139.133266	-16.916109	9.264589
-137.267303	-17.979575	9.274586
-135.476901	-17.400005	9.284583
-133.406925	-23.191598	9.294579
-131.615689	-15.207232	9.304576
-129.873002	-17.065722	9.314573
-127.955534	-17.431643	9.324570
-125.763001	-24.666931	9.334567
-124.048766	-10.293192	9.344563
-122.229136	-19.363629	9.354560
-120.547565	-26.602640	9.364557
-118.476168	-23.140659	9.374554
-116.680512	-20.312016	9.384551
-114.824659	-28.884561	9.394547
-112.780238	-24.909874	9.404544
-110.997262	-24.839077	9.414541
-109.197614	-22.991547	9.424538
-107.285071	-22.796165	9.434535
-105.189412	-16.499224	9.444531
-103.272710	-12.696769	9.454528
-101.740767	-24.820621	9.464525
-99.642458	-26.085334	9.474522
-97.696152	-19.145638	9.484519
-96.281179	-22.094922	9.494515
-94.210783	-22.665208	9.504512
-92.324765	-22.449793	9.514509
-90.473930	-17.981587	9.524506
-88.501467	-16.095300	9.534503
-86.700400	-19.608263	9.544499
-84.820488	-23.477999	9.554496
-82.742626	-19.124952	9.564493
-80.923647	-23.877029	9.574490
-79.010904	-29.490339	9.584487
-77.386109	-21.056238	9.594483
-75.387654	-25.105925	9.604480
-73.414203	-24.369206	9.614477
-71.564967	-30.572351	9.624474
-69.757259	-22.922130	9.634471
-67.586286	-23.011094	9.644467
-66.088140	-23.805833	9.654464
-64.492549	-18.756908	9.664461
-62.441310	-21.454016	9.674458
-60.077218	-21.763248	9.684455
-58.489949	-12.588963	9.694451
-56.635691	-21.169113	9.704448
-54.718369	-15.989938	9.714445
-52.738159	-21.332955	9.724442
-50.799827	-20.887443	9.734439
-49.058129	-19.603754	9.744435
-47.206952	-17.172317	9.754432
-45.438372	-14.798751	9.764429
-43.454509	-18.096121	9.774426
-41.363135	-18.477086	9.784423
-39.852866	-18.762187	9.794419
-37.875462	-23.196891	9.804416
-36.035823	-21.463048	9.814413
-34.227807	-18.437374	9.824410
-32.101758	-25.695135	9.834407
-30.220817	-18.875998	9.844403
-28.353327	-19.879628	9.854400
-26.450867	-22.249828	9.864397
-24.976717	-27.722083	9.874394
-23.010180	-17.804629	9.884391
-20.765884	-20.960376	9.894387
-19.090721	-18.960292	9.904384
-17.226778	-20.487535	9.914381
-15.215485	-25.394975	9.924378
-13.390581	-24.182951	9.934375
-11.539545	-23.226136	9.944371
-9.739489	-24.818968	9.954368
-7.802560	-17.591920	9.964365
-6.156561	-23.964699	9.974362
-4.947120	-2.631156	9.984359
-3.647229	35.206262	9.994355
-2.489799	99.760784	10.004352
-1.026870	190.312384	10.014349
0.000000	248.454248	10.019354
0.576753	304.647811	10.024359
1.573047	338.546704	10.029363
1.910335	392.006619	10.034368
2.219178	408.830252	10.039373
3.254795	423.651994	10.044378
3.171529	465.368237	10.049383
3.569387	470.000837	10.054387
3.611845	497.878646	10.059392
3.895297	507.790097	10.064397
4.033108	520.005010	10.069402
3.909799	520.570314	10.074407
4.303509	526.584974	10.079411
4.312709	564.371265	10.084416
4.708403	542.846273	10.089421
4.545620	550.469862	10.094426
4.340404	565.953295	10.099431
4.747508	561.490342	10.104435
4.680895	566.933486	10.109440
4.652570	563.434104	10.114445
4.995762	566.254111	10.119450
4.680373	570.784478	10.124455
4.712885	564.662431	10.129459
4.761190	586.137174	10.134464
4.522310	577.795525	10.139469
5.048772	572.821530	10.144474
4.788611	583.228169	10.149479
4.884175	584.622717	10.154483
5.313240	600.864435	10.159488
4.994610	601.716360	10.164493
5.373063	606.317409	10.169498
5.099641	622.092474	10.174503
5.384194	627.886472	10.179507
5.283204	628.984376	10.184512
5.234935	629.941408	10.189517
5.403878	630.565753	10.194522
5.196760	626.848875	10.199527
5.197398	629.764536	10.204531
5.338550	620.971164	10.209536
5.610317	631.417566	10.214541
5.694469	640.290165	10.219546
5.738268	641.603090	10.224551
5.809170	630.067598	10.229555
5.665997	633.737895	10.234560
5.538660	630.590176	10.239565
5.822768	645.647139	10.244570
6.063469	665.134339	10.249575
6.107640	662.203681	10.254579
5.911583	662.580324	10.259584
5.835579	673.664118	10.264589
6.428118	680.221132	10.269594
6.039421	675.593352	10.274599
6.350547	684.065500	10.279603
6.318794	690.668485	10.284608
6.115507	678.690994	10.289613
6.413850	685.676556	10.294618
6.468812	690.931621	10.299623
6.467674	689.178272	10.304627
6.527927	686.416929	10.309632
6.477486	690.663799	10.314637
6.823875	692.327428	10.319642
6.675947	689.706524	10.324647
6.742237	683.932272	10.329651
6.645232	692.485296	10.334656
6.602369	709.786423	10.339661
6.833927	697.737977	10.344666
6.665921	686.281549	10.349671
7.016377	709.999566	10.354675
7.128678	703.211881	10.359680
6.598147	697.567516	10.364685
6.944522	696.797934	10.369690
7.035808	704.677541	10.374695
6.833951	706.479085	10.379699
6.823938	705.903544	10.384704
6.776528	712.920617	10.389709
7.042647	697.578742	10.394714
7.016805	722.213080	10.399719
7.106963	707.265112	10.404723
6.901305	722.187392	10.409728
7.008177	734.666038	10.414733
7.491275	737.752343	10.419738
7.186151	748.803357	10.424743
7.212038	740.452496	10.429747
7.404101	747.762545	10.434752
7.243268	761.014040	10.439757
7.364552	740.615888	10.444762
7.228590	755.441930	10.449767
7.448731	774.186662	10.454771
7.867705	786.104639	10.459776
7.856985	787.826819	10.464781
8.205366	772.982673	10.469786
8.036053	785.587419	10.474791
8.009103	786.137363	10.479795
8.140830	784.269768	10.484800
8.126829	790.963006	10.489805
7.985572	789.274573	10.494810
8.058857	790.078186	10.499815
8.371408	787.811165	10.504819
8.337750	793.619719	10.509824
8.312019	796.003458	10.514829
8.382133	793.024481	10.519834
8.228021	797.317881	10.524839
8.101755	793.769411	10.529843
8.336596	790.245343	10.534848
8.283637	786.038634	10.539853
8.469186	797.087110	10.544858
8.293006	812.733330	10.549863
8.297405	802.589716	10.554867
8.333974	796.457462	10.559872
8.188079	805.475666	10.564877
8.729765	809.355308	10.569882
8.548220	824.543505	10.574887
8.655751	829.892737	10.579891
8.766026	833.538426	10.584896
8.727218	837.334053	10.589901
8.830335	837.103160	10.594906
8.555118	850.680489	10.599911
8.895190	841.068354	10.604915
9.252191	845.065775	10.609920
8.788083	847.951533	10.614925
9.209827	838.502991	10.619930
9.253516	852.251802	10.624935
9.284837	843.029537	10.629939
9.424151	851.751541	10.634944
9.270693	850.143894	10.639949
9.475360	854.309118	10.644954
9.506406	862.679391	10.649959
9.523466	856.662188	10.654963
9.496287	848.972588	10.659968
9.733058	863.382893	10.664973
9.638717	844.586483	10.669978
9.727334	858.965223	10.674983
9.623018	861.416701	10.679987
9.579638	863.552531	10.684992
9.716672	886.768716	10.689997
10.199918	868.791625	10.695002
10.211552	883.263093	10.700007
10.089494	869.656106	10.705011
10.032497	855.619284	10.710016
9.771035	859.393662	10.715021
9.752985	857.499486	10.720026
9.910551	874.144365	10.725031
10.467322	879.716848	10.730035
10.224294	886.230620	10.735040
10.140550	890.635826	10.740045
10.064166	887.568233	10.745050
9.957681	901.892980	10.750055
10.068422	891.339679	10.755059
10.600524	891.351019	10.760064
10.012282	890.927629	10.765069
10.300368	892.611620	10.770074
10.374901	898.888662	10.775079
10.702236	882.817734	10.780083
10.441672	898.725089	10.785088
10.609983	891.729685	10.790093
10.952373	901.922167	10.795098
10.356736	899.205481	10.800103
10.635117	907.008045	10.805107
11.008431	913.286321	10.810112
10.733180	922.000377	10.815117
10.909754	913.527609	10.820122
10.992646	925.541888	10.825127
10.992704	918.295764	10.830131
11.085078	936.797734	10.835136
11.000773	934.691766	10.840141
11.151394	920.148675	10.845146
11.109733	924.586603	10.850151
11.422195	913.878105	10.855155
11.295733	924.118581	10.860160
11.255038	934.452617	10.865165
11.781091	925.233387	10.870170
11.601270	923.081154	10.875175
11.610047	921.026572	10.880179
11.527088	914.426054	10.885184
11.502277	920.323134	10.890189
11.994956	922.412890	10.895194
11.945229	921.895715	10.900199
11.758673	931.172796	10.905203
11.826542	925.464429	10.910208
11.832130	925.788413	10.915213
11.925612	929.118259	10.920218
11.732300	930.229334	10.925223
11.914380	931.818275	10.930227
11.864458	934.049776	10.935232
11.887964	932.989483	10.940237
12.109102	920.792703	10.945242
11.737564	930.627572	10.950247
12.044510	927.050969	10.955251
12.283529	931.929832	10.960256
11.727842	941.057641	10.965261
11.524010	928.663711	10.970266
11.980253	936.887355	10.975271
12.416029	935.638298	10.980275
12.207533	948.713063	10.985280
12.170206	967.439190	10.990285
12.641935	955.883658	10.995290
12.527678	974.618911	11.000295
12.529107	971.430078	11.005299
12.629103	969.799335	11.010304
12.321221	969.059983	11.015309
12.146064	973.334714	11.020314
12.299725	971.364249	11.025319
12.468538	978.334344	11.030323
12.614418	970.978201	11.035328
12.499213	983.788956	11.040333
12.790787	982.651206	11.045338
13.284992	994.705592	11.050343
13.071541	1005.470938	11.055347
13.238467	1000.579381	11.060352
13.216097	996.643701	11.065357
13.129582	989.294655	11.070362
13.038852	1001.828706	11.075367
13.461782	999.192383	11.080371
13.297889	1001.118795	11.085376
13.204108	1015.821678	11.090381
13.444228	995.724337	11.095386
13.265589	999.137029	11.100391
13.350889	1002.597509	11.105395
13.622473	1003.533508	11.110400
13.704867	1015.076427	11.115405
13.461314	1012.562181	11.120410
13.502487	1014.176761	11.125415
13.646726	1008.082438	11.130419
13.435929	1009.918561	11.135424
13.638997	1011.609820	11.140429
13.801644	1002.159923	11.145434
13.598969	1011.319777	11.150439
13.490559	996.658654	11.155443
13.505581	1002.317599	11.160448
13.631969	1008.546993	11.165453
13.840763	1017.513483	11.170458
14.118530	1039.753399	11.175463
14.103850	1033.979308	11.180467
14.491191	1037.423157	11.185472
14.497794	1034.982547	11.190477
14.433979	1015.321595	11.195482
14.240489	1008.109452	11.200487
14.256198	1010.273726	11.205491
14.491275	1011.316475	11.210496
14.299537	1007.584428	11.215501
14.677427	995.903483	11.220506
14.289734	1011.799700	11.225511
14.361065	1006.981737	11.230515
14.752626	1026.115774	11.235520
14.190671	1036.135630	11.240525
14.708752	1047.602772	11.245530
14.577972	1037.389091	11.250535
14.530068	1042.695386	11.255539
15.032663	1043.275991	11.260544
14.697572	1032.225991	11.265549
14.931333	1045.078909	11.270554
14.664863	1044.157903	11.275559
14.766925	1041.851878	11.280563
15.318239	1038.548510	11.285568
14.991124	1046.085028	11.290573
15.022562	1040.366657	11.295578
15.109334	1045.279305	11.300583
15.011748	1037.526718	11.305587
15.052197	1036.559910	11.310592
14.973611	1046.639869	11.315597
15.436599	1048.343291	11.320602
15.087676	1052.115898	11.325607
14.982484	1050.979930	11.330611
15.467769	1059.386673	11.335616
15.205029	1067.534262	11.340621
15.589023	1061.330709	11.345626
15.245229	1069.600040	11.350631
15.323926	1080.613737	11.355635
15.392246	1059.501329	11.360640
15.248787	1077.085449	11.365645
15.322663	1062.276910	11.370650
15.484911	1095.149969	11.375655
15.456841	1091.260905	11.380659
15.707749	1091.630919	11.385664
15.411263	1100.607093	11.390669
16.015900	1101.169848	11.395674
16.020677	1097.814870	11.400679
15.909207	1103.736886	11.405683
16.140863	1101.378641	11.410688
15.738552	1103.838268	11.415693
16.214005	1105.061883	11.420698
16.475276	1119.178372	11.425703
16.401441	1124.514064	11.430707
16.770043	1097.469981	11.435712
16.376436	1097.780372	11.440717
16.616669	1084.881806	11.445722
16.491180	1096.093667	11.450727
16.579012	1092.041033	11.455731
16.631633	1089.807543	11.460736
16.558257	1100.580579	11.465741
16.636992	1083.319039	11.470746
16.585991	1098.224920	11.475751
16.521168	1093.586344	11.480755
16.935767	1103.589253	11.485760
16.509011	1100.142255	11.490765
17.004552	1123.689574	11.495770
17.094975	1118.165195	11.500775
16.903041	1124.538456	11.505779
17.091873	1108.547720	11.510784
16.959912	1116.068915	11.515789
17.374159	1118.019821	11.520794
16.991368	1119.115401	11.525799
17.160400	1113.494905	11.530803
17.048566	1112.604423	11.535808
17.442406	1119.710585	11.540813
17.633740	1114.652667	11.545818
17.345722	1110.790868	11.550823
17.329046	1119.083745	11.555827
17.461301	1125.017357	11.560832
17.271430	1131.945391	11.565837
17.324166	1117.269480	11.570842
17.666539	1129.969529	11.575847
17.543465	1133.840176	11.580851
17.597748	1129.091125	11.585856
17.416532	1131.491836	11.590861
17.765441	1123.248505	11.595866
17.108338	1139.999981	11.600871
17.281653	1129.116398	11.605875
17.536125	1131.453921	11.610880
17.485551	1145.711642	11.615885
18.089586	1149.655553	11.620890
17.956858	1163.245138	11.625895
18.252120	1156.538447	11.630899
18.615707	1165.319486	11.635904
18.055625	1158.979467	11.640909
18.196463	1159.272422	11.645914
18.262161	1155.630163	11.650919
18.169975	1155.641735	11.655923
18.088526	1165.149787	11.660928
17.938150	1166.217760	11.665933
18.386230	1157.398761	11.670938
18.331757	1162.841769	11.675943
18.467349	1168.629784	11.680947
18.705530	1164.980512	11.685952
18.592388	1164.844036	11.690957
18.835503	1172.122502	11.695962
18.380419	1166.191520	11.700967
18.619837	1160.668590	11.705971
18.698834	1166.322126	11.710976
18.413929	1179.825611	11.715981
18.499245	1162.408382	11.720986
18.443950	1174.004930	11.725991
18.614196	1200.900168	11.730995
19.174531	1187.633478	11.736000
19.242134	1195.829375	11.741005
19.326480	1194.606390	11.746010
19.318714	1195.533344	11.751015
19.467043	1177.117273	11.756019
19.463038	1172.344389	11.761024
19.367592	1169.932650	11.766029
19.509831	1168.104332	11.771034
19.034026	1172.707780	11.776039
19.027714	1172.658345	11.781043
19.229892	1165.897109	11.786048
19.029491	1174.052162	11.791053
19.369669	1186.404096	11.796058
19.629344	1191.905818	11.801063
19.931424	1206.774416	11.806067
19.672048	1195.089301	11.811072
19.441943	1193.038090	11.816077
19.386536	1206.028741	11.821082
19.553006	1195.706032	11.826087
19.130840	1198.787022	11.831091
19.588709	1202.134504	11.836096
19.622255	1205.492898	11.841101
19.811143	1201.692203	11.846106
20.082498	1215.264693	11.851111
20.140397	1209.944167	11.856115
20.341694	1206.974144	11.861120
20.000478	1202.729712	11.866125
20.341485	1199.106609	11.871130
20.221880	1196.490555	11.876135
19.898623	1195.709487	11.881139
20.127769	1215.569866	11.886144
20.098672	1224.277955	11.891149
20.704216	1222.273226	11.896154
20.431854	1246.209742	11.901159
20.457282	1242.239562	11.906163
20.804501	1220.618797	11.911168
20.645433	1231.170627	11.916173
20.603922	1213.291006	11.921178
20.434200	1217.902418	11.926183
20.890117	1221.761163	11.931187
20.649510	1225.803550	11.936192
20.749217	1216.030808	11.941197
20.833105	1219.184051	11.946202
20.735051	1228.084496	11.951207
21.100063	1224.900693	11.956211
21.275257	1220.993365	11.961216
21.109554	1223.194491	11.966221
20.962097	1222.289184	11.971226
20.979460	1223.175860	11.976231
20.839083	1229.947807	11.981235
20.928617	1219.638931	11.986240
20.958775	1236.720876	11.991245
21.193152	1217.985091	11.996250
21.052794	1235.769187	12.001255
20.745650	1237.562356	12.006259
20.983844	1225.312137	12.011264
20.922805	1238.246943	12.016269
21.306132	1245.350114	12.021274
21.450145	1251.879585	12.026279
21.453054	1251.355580	12.031283
21.792000	1263.130596	12.036288
21.566222	1266.787418	12.041293
21.514077	1250.297207	12.046298
21.559040	1269.485274	12.051303
21.278573	1254.170071	12.056307
21.678155	1250.141786	12.061312
21.416409	1245.722234	12.066317
21.517387	1230.343059	12.071322
21.418462	1231.973702	12.076327
21.234098	1240.362782	12.081331
21.706101	1246.846243	12.086336
21.379862	1240.760632	12.091341
21.365686	1226.861704	12.096346
21.620258	1237.647189	12.101351
21.517781	1247.112916	12.106355
21.580089	1235.114677	12.111360
21.308498	1223.526106	12.116365
21.345872	1233.355881	12.121370
21.577425	1236.077132	12.126375
21.287959	1231.941134	12.131379
21.692918	1236.943448	12.136384
21.211957	1234.623152	12.141389
21.381445	1228.319700	12.146394
21.584959	1258.800557	12.151399
21.699303	1258.752376	12.156403
21.291795	1238.385830	12.161408
21.476519	1233.537089	12.166413
21.509186	1229.639877	12.171418
21.325269	1237.352353	12.176423
21.521574	1232.132749	12.181427
21.494682	1232.592811	12.186432
21.494538	1236.693043	12.191437
21.664325	1229.936944	12.196442
21.640567	1230.555783	12.201447
21.615950	1238.610291	12.206451
21.654030	1241.234667	12.211456
21.421453	1244.151380	12.216461
21.953815	1241.387171	12.221466
21.572368	1228.155543	12.226471
21.603468	1248.719356	12.231475
21.901724	1238.714651	12.236480
21.254839	1246.087805	12.241485
21.800803	1239.889883	12.246490
21.905099	1237.889408	12.251495
21.363291	1216.109248	12.256499
21.586349	1201.027607	12.261504
20.987094	1211.080340	12.266509
21.510235	1217.375854	12.271514
21.567162	1230.706587	12.276519
21.539415	1231.234596	12.281523
21.692953	1223.331464	12.286528
21.070434	1214.646927	12.291533
21.289754	1208.909560	12.296538
21.494607	1237.360569	12.301543
21.459336	1237.019278	12.306547
21.563542	1224.112323	12.311552
21.162341	1232.225318	12.316557
22.134919	1238.507502	12.321562
21.572711	1225.550720	12.326567
21.424961	1217.725611	12.331571
21.494326	1213.437763	12.336576
21.297273	1217.742866	12.341581
21.433885	1212.173236	12.346586
21.471763	1215.105153	12.351591
21.254229	1217.312969	12.356595
21.419864	1218.075067	12.361600
21.183887	1220.008274	12.366605
21.425669	1223.180489	12.371610
21.612059	1239.117852	12.376615
21.650575	1239.856071	12.381619
21.678476	1221.094868	12.386624
21.142575	1217.359313	12.391629
21.435511	1216.640811	12.396634
21.449985	1218.224978	12.401639
21.273879	1221.465426	12.406643
21.668349	1226.409482	12.411648
21.489482	1228.923377	12.416653
21.901967	1222.524396	12.421658
21.569281	1228.659949	12.426663
21.417995	1220.059521	12.431667
21.430704	1221.863173	12.436672
21.241349	1231.680224	12.441677
21.487137	1212.833813	12.446682
21.164786	1220.489512	12.451687
21.020315	1219.966938	12.456691
21.379598	1245.097413	12.461696
21.506432	1240.847701	12.466701
21.725140	1240.945304	12.471706
21.497778	1232.279731	12.476711
21.119198	1229.430583	12.481715
21.550662	1243.349731	12.486720
21.400883	1243.507688	12.491725
21.459397	1228.668313	12.496730
21.785700	1239.969074	12.501735
22.017796	1236.961015	12.506739
21.691519	1222.343876	12.511744
21.366052	1224.904809	12.516749
21.689929	1222.703727	12.521754
21.475976	1230.528227	12.526759
21.447750	1228.101025	12.531763
21.740388	1221.700659	12.536768
21.633988	1234.656891	12.541773
21.621354	1228.235828	12.546778
21.617008	1226.434038	12.551783
21.461036	1238.429906	12.556787
21.544742	1222.228726	12.561792
21.498655	1223.551311	12.566797
21.615767	1240.166793	12.571802
21.797358	1232.702317	12.576807
21.669140	1222.276779	12.581811
21.437515	1210.254480	12.586816
21.421470	1209.001775	12.591821
21.459155	1196.275770	12.596826
21.250166	1183.082910	12.601831
21.153594	1198.325753	12.606835
21.368593	1205.269669	12.611840
21.161396	1221.263483	12.616845
21.406925	1226.119330	12.621850
21.735649	1226.390202	12.626855
21.642281	1236.777011	12.631859
21.895902	1224.465982	12.636864
21.489530	1217.101605	12.641869
21.191073	1211.866306	12.646874
21.488477	1199.471043	12.651879
21.591977	1194.994824	12.656883
21.701030	1193.146565	12.661888
21.307136	1197.550870	12.666893
21.343103	1196.015474	12.671898
21.443874	1201.809057	12.676903
21.531819	1201.269912	12.681907
21.736478	1200.570222	12.686912
21.286583	1197.803420	12.691917
21.473042	1206.275262	12.696922
21.521967	1212.099197	12.701927
21.539963	1200.984861	12.706931
21.722370	1205.781383	12.711936
21.475892	1205.219884	12.716941
21.669710	1202.541221	12.721946
21.375948	1202.461940	12.726951
21.305273	1209.139180	12.731955
21.635736	1194.505626	12.736960
21.590906	1201.284398	12.741965
21.532934	1203.438375	12.746970
21.483295	1205.236200	12.751975
21.588372	1203.278184	12.756979
21.548334	1195.435906	12.761984
21.096846	1197.537529	12.766989
21.522304	1205.834051	12.771994
21.230702	1219.658770	12.776999
21.236802	1198.349498	12.782003
21.656569	1200.545546	12.787008
21.422064	1203.927772	12.792013
21.364895	1198.731263	12.797018
21.319604	1207.435617	12.802023
21.461906	1210.423419	12.807027
21.664446	1211.706346	12.812032
21.254062	1209.195020	12.817037
21.614569	1199.344419	12.822042
21.498885	1194.466336	12.827047
21.379842	1208.173631	12.832051
21.631057	1205.641935	12.837056
21.601888	1208.324341	12.842061
21.772711	1206.133482	12.847066
21.692260	1204.310717	12.852071
21.422378	1210.991346	12.857075
21.797436	1196.271829	12.862080
21.595550	1207.898094	12.867085
21.379813	1215.972035	12.872090
21.544498	1204.676600	12.877095
21.494195	1190.302486	12.882099
21.555023	1202.629605	12.887104
21.428028	1186.670236	12.892109
21.219934	1183.164684	12.897114
21.520371	1202.982135	12.902119
21.570694	1191.965155	12.907123
21.739289	1178.426636	12.912128
21.110933	1177.358335	12.917133
21.185978	1175.506040	12.922138
21.660732	1201.132120	12.927143
21.471416	1204.754725	12.932147
21.650905	1202.929923	12.937152
21.283262	1184.736496	12.942157
21.344443	1190.394460	12.947162
21.441821	1208.689395	12.952167
21.521467	1207.229034	12.957171
21.640673	1194.906353	12.962176
21.124053	1192.629600	12.967181
21.382015	1198.279835	12.972186
21.499958	1211.181338	12.977191
21.464101	1206.820387	12.982195
21.710331	1209.387902	12.987200
21.385750	1192.203179	12.992205
21.570052	1191.673897	12.997210
21.197333	1192.212774	13.002215
21.239128	1196.571240	13.007219
21.836631	1204.304141	13.012224
21.166210	1206.849128	13.017229
21.432460	1209.757233	13.022234
21.625859	1212.621765	13.027239
21.454667	1214.549369	13.032243
21.849834	1201.261702	13.037248
21.680245	1189.718392	13.042253
21.267794	1182.976336	13.047258
21.277420	1184.543926	13.052263
21.252958	1180.094431	13.057267
21.553225	1176.857887	13.062272
21.093608	1179.006537	13.067277
21.473728	1198.330289	13.072282
21.677594	1203.739991	13.077287
21.194248	1207.488346	13.082291
21.602172	1206.770426	13.087296
21.493315	1209.951257	13.092301
21.816938	1195.866010	13.097306
21.484270	1192.161125	13.102311
21.311434	1187.992343	13.107315
21.474220	1179.573661	13.112320
21.188010	1193.816974	13.117325
21.559717	1184.172760	13.122330
21.434886	1183.339541	13.127335
21.307209	1190.497384	13.132339
21.113829	1192.918968	13.137344
21.345485	1211.432191	13.142349
21.398177	1202.960091	13.147354
21.849138	1214.332414	13.152359
21.358647	1220.316511	13.157363
21.637011	1212.231044	13.162368
21.521450	1226.798840	13.167373
21.553187	1207.133425	13.172378
21.625716	1182.101342	13.177383
21.388801	1174.413483	13.182387
21.469445	1188.617200	13.187392
21.419437	1187.292642	13.192397
21.421290	1185.915655	13.197402
21.596167	1192.304556	13.202407
21.362033	1190.217717	13.207411
21.437618	1177.733271	13.212416
21.208496	1186.457473	13.217421
21.444633	1193.275006	13.222426
21.404370	1187.000297	13.227431
21.598278	1196.454986	13.232435
21.389532	1191.482935	13.237440
21.383109	1187.921560	13.242445
21.860265	1181.688905	13.247450
21.835333	1188.992788	13.252455
21.321781	1190.656445	13.257459
21.897596	1178.491188	13.262464
21.557659	1182.118889	13.267469
21.333394	1188.391676	13.272474
21.199890	1192.109457	13.277479
21.263338	1194.333954	13.282483
21.566014	1186.219391	13.287488
21.418323	1186.894267	13.292493
21.485672	1184.434481	13.297498
21.507781	1180.584698	13.302503
21.187137	1191.789913	13.307507
21.511199	1184.398933	13.312512
21.610459	1181.438882	13.317517
21.267105	1179.202305	13.322522
21.476645	1188.283904	13.327527
21.376291	1192.078401	13.332531
21.444176	1186.352582	13.337536
21.273880	1191.831421	13.342541
21.375329	1179.420121	13.347546
21.599831	1185.463627	13.352551
21.438263	1189.986995	13.357555
21.857447	1178.343473	13.362560
21.596687	1192.060742	13.367565
21.681859	1193.269346	13.372570
21.691826	1195.548106	13.377575
21.478957	1191.915578	13.382579
21.585379	1196.508168	13.387584
21.398846	1203.276427	13.392589
21.606218	1197.238188	13.397594
21.535195	1192.173204	13.402599
21.443630	1186.332466	13.407603
21.696702	1195.711485	13.412608
21.430477	1196.851556	13.417613
21.489780	1196.766422	13.422618
21.560259	1198.152416	13.427623
21.309562	1192.942622	13.432627
21.494690	1189.934180	13.437632
21.197947	1199.279471	13.442637
21.207031	1204.122561	13.447642
21.680247	1197.723366	13.452647
21.230834	1212.631411	13.457651
21.320096	1208.870261	13.462656
21.507795	1215.462135	13.467661
21.785866	1211.502129	13.472666
21.498662	1200.258276	13.477671
21.266630	1208.484626	13.482675
21.755955	1193.628610	13.487680
21.412722	1202.249595	13.492685
21.592420	1202.561583	13.497690
22.059754	1201.397361	13.502695
21.417397	1199.454484	13.507699
21.429154	1176.936366	13.512704
21.256633	1180.877992	13.517709
21.619968	1180.238150	13.522714
21.228611	1188.160312	13.527719
21.214842	1195.727353	13.532723
21.592127	1204.624506	13.537728
21.465431	1212.750476	13.542733
21.403554	1204.870675	13.547738
21.620771	1204.774546	13.552743
21.356529	1209.044631	13.557747
21.622577	1203.670406	13.562752
21.511329	1190.843580	13.567757
21.460887	1182.815307	13.572762
21.561389	1182.881301	13.577767
21.324920	1183.106702	13.582771
21.706283	1168.647987	13.587776
21.307770	1180.050121	13.592781
21.163507	1187.800402	13.597786
21.401102	1188.727643	13.602791
21.214443	1211.638006	13.607795
21.854906	1199.675313	13.612800
21.526625	1210.181576	13.617805
21.261507	1182.651775	13.622810
21.097309	1185.026125	13.627815
20.992274	1208.183665	13.632819
21.404684	1199.441296	13.637824
21.368279	1203.271329	13.642829
21.694571	1208.453341	13.647834
21.747801	1216.344028	13.652839
21.516583	1211.064887	13.657843
21.286078	1209.616148	13.662848
21.171256	1215.701175	13.667853
21.346801	1211.262347	13.672858
21.430574	1215.817555	13.677863
21.001309	1216.149404	13.682867
21.527227	1213.329456	13.687872
21.684120	1213.840629	13.692877
21.632012	1219.377900	13.697882
21.571660	1211.641358	13.702887
21.402118	1220.885947	13.707891
21.795490	1216.451798	13.712896
21.432376	1222.068640	13.717901
21.544230	1218.430042	13.722906
21.617965	1216.111161	13.727911
21.318581	1218.414036	13.732915
21.458618	1199.067257	13.737920
21.511021	1215.571605	13.742925
21.467793	1222.378517	13.747930
21.363631	1228.263148	13.752935
21.405140	1225.692355	13.757939
21.670478	1216.486144	13.762944
21.400246	1218.789100	13.767949
21.324097	1226.399224	13.772954
21.623472	1228.194999	13.777959
21.239931	1214.457503	13.782963
21.528633	1225.062489	13.787968
21.440366	1233.855718	13.792973
21.658531	1222.507583	13.797978
21.892586	1216.531313	13.802983
21.315068	1210.823272	13.807987
21.596603	1188.117022	13.812992
21.199054	1194.378027	13.817997
21.363129	1191.368212	13.823002
21.261476	1199.586377	13.828007
21.395216	1216.771628	13.833011
21.807525	1220.454397	13.838016
21.291893	1206.864136	13.843021
21.411032	1199.549991	13.848026
21.487243	1202.067350	13.853031
21.368685	1219.947300	13.858035
21.557566	1219.841498	13.863040
21.366247	1205.642830	13.868045
21.635138	1210.684185	13.873050
21.468544	1195.830285	13.878055
21.448404	1199.555218	13.883059
21.544504	1192.795121	13.888064
21.413896	1184.763863	13.893069
21.265817	1179.892528	13.898074
21.357363	1191.074575	13.903079
21.574596	1195.860807	13.908083
21.785921	1183.834110	13.913088
21.794347	1193.354653	13.918093
21.184435	1191.332484	13.923098
21.706443	1194.437917	13.928103
21.534273	1197.848046	13.933107
21.510007	1188.194447	13.938112
21.693013	1189.628725	13.943117
21.436413	1195.815208	13.948122
21.770961	1188.488786	13.953127
21.313512	1197.167411	13.958131
21.460041	1183.935189	13.963136
21.175577	1191.852918	13.968141
21.438261	1187.893796	13.973146
21.819539	1193.194769	13.978151
21.309968	1194.960296	13.983155
21.456873	1173.797338	13.988160
21.291630	1187.570332	13.993165
21.163334	1198.120383	13.998170
21.447975	1192.793661	14.003175
21.466326	1199.545007	14.008179
21.507585	1191.219821	14.013184
21.316596	1197.378492	14.018189
21.400055	1191.979938	14.023207
21.197653	1186.783701	14.028224
20.868355	1200.075916	14.033242
21.489327	1196.841963	14.038259
21.606255	1210.794443	14.043277
21.526185	1219.725976	14.048295
21.826101	1221.988853	14.053312
21.530207	1205.471125	14.058330
21.545108	1191.662827	14.063347
21.523351	1193.012779	14.068365
21.630779	1204.225086	14.073383
21.623745	1207.743388	14.078400
21.750990	1224.421764	14.083418
21.470633	1218.629210	14.088435
21.839643	1227.570911	14.093453
21.533844	1238.297043	14.098471
21.693658	1233.776018	14.103488
21.337452	1230.317265	14.108506
21.998788	1232.014425	14.113523
21.577792	1232.487424	14.118541
21.532799	1229.881916	14.123559
21.985970	1227.568170	14.128576
21.717606	1235.422375	14.133594
21.670837	1239.178249	14.138611
21.947007	1232.140785	14.143629
22.045749	1218.577056	14.148647
22.105524	1235.906406	14.153664
21.965792	1237.330234	14.158682
22.144401	1231.255261	14.163699
21.550618	1241.423309	14.168717
21.543510	1231.591814	14.173735
21.884623	1226.507063	14.178752
21.717790	1238.397050	14.183770
21.879779	1237.922936	14.188787
21.668610	1239.889823	14.193805
22.117901	1254.470428	14.198823
22.364583	1259.069805	14.203840
22.125568	1266.511944	14.208858
22.318928	1245.430006	14.213875
22.191037	1239.927719	14.218893
22.165837	1236.702447	14.223911
22.378724	1232.539460	14.228928
22.070803	1240.360653	14.233946
21.982945	1229.272650	14.238963
22.129914	1246.662035	14.243981
22.223730	1256.471888	14.248999
22.664255	1254.965517	14.254016
22.381185	1252.056644	14.259034
22.309788	1233.160918	14.264051
22.057639	1238.475335	14.269069
22.084526	1262.801828	14.274087
22.194917	1256.064492	14.279104
22.130891	1271.280678	14.284122
22.080012	1266.577753	14.289139
22.459623	1263.132181	14.294157
22.111900	1266.398109	14.299175
22.373959	1267.279667	14.304192
22.262849	1273.063941	14.309210
22.532441	1262.532359	14.314227
22.800249	1273.061633	14.319245
22.486939	1268.243268	14.324263
22.572979	1273.925312	14.329280
22.177303	1280.088450	14.334298
22.261313	1270.489352	14.339315
22.253683	1282.253310	14.344333
22.400466	1293.805463	14.349351
22.909799	1298.189930	14.354368
22.858847	1296.044671	14.359386
22.475689	1293.030634	14.364403
22.701485	1297.457181	14.369421
22.697386	1307.542228	14.374439
22.885429	1295.741650	14.379456
22.674373	1302.430611	14.384474
22.954315	1305.590139	14.389491
22.845938	1298.665889	14.394509
22.900261	1297.334370	14.399527
23.141115	1283.842292	14.404544
22.785428	1285.709544	14.409562
22.751545	1276.058463	14.414579
22.649965	1279.642199	14.419597
22.674766	1292.443876	14.424615
22.824649	1296.852644	14.429632
22.878327	1301.391586	14.434650
23.151890	1293.412294	14.439667
22.830689	1295.653135	14.444685
22.775363	1301.359311	14.449703
23.295949	1297.262053	14.454720
23.042864	1301.543195	14.459738
23.235216	1296.677197	14.464755
23.330104	1293.849598	14.469773
23.214022	1299.823433	14.474791
23.256826	1296.362365	14.479808
23.201651	1300.615084	14.484826
23.011450	1308.747862	14.489843
23.052492	1311.627756	14.494861
22.866555	1307.180734	14.499879
23.264948	1302.204794	14.504896
23.086730	1310.537002	14.509914
23.345455	1295.668851	14.514931
23.153849	1307.153870	14.519949
23.308453	1303.185771	14.524967
23.775560	1292.004482	14.529984
23.269132	1303.201523	14.535002
23.279485	1301.180188	14.540019
23.341909	1285.125871	14.545037
23.233801	1297.374616	14.550055
23.035402	1298.346924	14.555072
22.926613	1295.718547	14.560090
23.284050	1298.949082	14.565107
23.453612	1291.900280	14.570125
23.180866	1303.940917	14.575143
23.247144	1306.524210	14.580160
23.590848	1317.100398	14.585178
23.479663	1332.788200	14.590195
23.500237	1333.637496	14.595213
23.664011	1326.790943	14.600231
23.894412	1325.467515	14.605248
24.093598	1327.383117	14.610266
23.661096	1307.340774	14.615283
23.924412	1295.307973	14.620301
23.757093	1303.035989	14.625319
23.810689	1293.013877	14.630336
23.682894	1302.049025	14.635354
23.754152	1293.414609	14.640371
23.851910	1286.238841	14.645389
23.499264	1305.524777	14.650407
23.752090	1295.923903	14.655424
23.391255	1301.917903	14.660442
23.501990	1321.585326	14.665459
23.838793	1329.157442	14.670477
24.113028	1338.520160	14.675495
23.999692	1332.988774	14.680512
24.086595	1328.798665	14.685530
23.870937	1331.442663	14.690547
24.119110	1327.668839	14.695565
23.806500	1331.574103	14.700583
24.186974	1323.156183	14.705600
24.063318	1333.261890	14.710618
24.340064	1327.806710	14.715635
24.062286	1304.636198	14.720653
23.799907	1299.743633	14.725671
23.877883	1318.870454	14.730688
24.053842	1316.814836	14.735706
24.163886	1320.396286	14.740723
24.336512	1319.720705	14.745741
24.097248	1332.429260	14.750759
24.319400	1325.247789	14.755776
24.301180	1327.356939	14.760794
24.048699	1327.048030	14.765811
24.256342	1319.821686	14.770829
24.299076	1325.034044	14.775847
24.390286	1313.094746	14.780864
24.284695	1321.528632	14.785882
24.293560	1318.090275	14.790899
24.477726	1313.392313	14.795917
24.175068	1321.799432	14.800935
24.525228	1314.031274	14.805952
24.850371	1322.140060	14.810970
24.529843	1320.906081	14.815987
24.758313	1315.167604	14.821005
24.684307	1321.027774	14.826023
24.609857	1315.321883	14.831040
24.519827	1325.879960	14.836058
24.337817	1320.375263	14.841075
24.435557	1313.226225	14.846093
24.320712	1320.996216	14.851111
24.527508	1319.948679	14.856128
24.420880	1321.387683	14.861146
24.541055	1329.200413	14.866163
24.676693	1312.362055	14.871181
24.373600	1322.650528	14.876199
24.651878	1319.770077	14.881216
24.539248	1315.616517	14.886234
24.579397	1314.955775	14.891251
24.954109	1318.943308	14.896269
24.295166	1328.689240	14.901287
24.665903	1325.235631	14.906304
24.613215	1340.406038	14.911322
24.685755	1359.201093	14.916339
25.019350	1345.939550	14.921357
25.006445	1353.457351	14.926375
25.068182	1348.234653	14.931392
25.286453	1351.831881	14.936410
25.001087	1351.169576	14.941427
25.231104	1336.968188	14.946445
24.896119	1331.937760	14.951463
24.813273	1330.385877	14.956480
25.029574	1340.638707	14.961498
25.016202	1343.967722	14.966515
25.096761	1348.167346	14.971533
25.073154	1352.319094	14.976551
25.160582	1357.124796	14.981568
25.119990	1352.742663	14.986586
25.070696	1365.218032	14.991603
25.162513	1357.255110	14.996621
25.011199	1363.983332	15.001639
25.182272	1348.528227	15.006656
25.467811	1344.440134	15.011674
25.156113	1356.749715	15.016691
25.326017	1354.080021	15.021709
25.535757	1349.797956	15.026727
25.196602	1353.531285	15.031744
25.598688	1350.313338	15.036762
25.265901	1355.412576	15.041779
25.645373	1355.863290	15.046797
25.485865	1351.751803	15.051815
25.380564	1345.059841	15.056832
25.348878	1344.317749	15.061850
24.904212	1354.938704	15.066867
25.491345	1349.155589	15.071885
25.577789	1357.901776	15.076903
25.279885	1359.100740	15.081920
25.535898	1341.005208	15.086938
25.370248	1348.648040	15.091955
26.011612	1357.385937	15.096973
25.881623	1361.173993	15.101991
25.760283	1351.857700	15.107008
25.698149	1351.966730	15.112026
25.535379	1363.813700	15.117043
25.708212	1354.260153	15.122061
25.520996	1355.416294	15.127079
25.852316	1372.527893	15.132096
25.884245	1381.874233	15.137114
26.171731	1380.956964	15.142131
26.162203	1363.776767	15.147149
25.716596	1369.699374	15.152167
25.615783	1352.535324	15.157184
25.887844	1357.854257	15.162202
25.887439	1358.670723	15.167219
25.883598	1373.260806	15.172237
25.996029	1378.123874	15.177255
26.004082	1383.258417	15.182272
26.264520	1381.713120	15.187290
25.996182	1373.604721	15.192307
26.548839	1358.873660	15.197325
26.254936	1352.784345	15.202343
26.101065	1346.251136	15.207360
26.138790	1344.368570	15.212378
26.258176	1342.364443	15.217395
25.895492	1345.030321	15.222413
26.097339	1346.590008	15.227431
26.074314	1353.530564	15.232448
26.094740	1357.052387	15.237466
26.156587	1371.246609	15.242483
26.509970	1372.066419	15.247501
26.468933	1376.925651	15.252519
26.329292	1373.308053	15.257536
26.726599	1374.888474	15.262554
26.636257	1370.006197	15.267571
26.700922	1350.558518	15.272589
26.539454	1343.296658	15.277607
26.419234	1333.506730	15.282624
26.187120	1342.720559	15.287642
26.430227	1342.957076	15.292659
26.637268	1331.752746	15.297677
26.374768	1341.723308	15.302695
26.188648	1362.022499	15.307712
26.654255	1369.039277	15.312730
26.630783	1371.762737	15.317747
26.549548	1368.991529	15.322765
26.208397	1375.745317	15.327783
26.212823	1376.586181	15.332800
26.836771	1371.328855	15.337818
26.614778	1371.326533	15.342835
26.585177	1375.992037	15.347853
26.779872	1373.703767	15.352871
26.786339	1376.345376	15.357888
26.843815	1378.805820	15.362906
26.590650	1370.959263	15.367923
26.827031	1377.716886	15.372941
26.591577	1378.526800	15.377959
26.842028	1383.548750	15.382976
26.884585	1390.253926	15.387994
26.669787	1405.050718	15.393011
26.990855	1398.537683	15.398029
27.220209	1413.494870	15.403047
26.952627	1412.806130	15.408064
27.225354	1402.434393	15.413082
27.001568	1412.490061	15.418099
27.396386	1406.830405	15.423117
27.353999	1401.495311	15.428135
27.041633	1384.213959	15.433152
27.201210	1380.061007	15.438170
27.006770	1401.950299	15.443187
27.148592	1395.327433	15.448205
27.586882	1397.233221	15.453223
27.215472	1388.636323	15.458240
27.482823	1387.635751	15.463258
27.425802	1393.458635	15.468275
27.419785	1386.868792	15.473293
27.247796	1384.532044	15.478311
27.278522	1379.790897	15.483328
27.489139	1385.199864	15.488346
27.139816	1388.420457	15.493363
27.536738	1394.260596	15.498381
27.282806	1402.260449	15.503399
27.355889	1409.221881	15.508416
27.560168	1407.100388	15.513434
27.207611	1409.100860	15.518451
27.416616	1394.923215	15.523469
27.876674	1403.012101	15.528487
27.679184	1406.268254	15.533504
27.669949	1397.209324	15.538522
27.700920	1408.007703	15.543539
27.704819	1397.408293	15.548557
27.745091	1407.577566	15.553575
27.506845	1410.166980	15.558592
27.947713	1403.273047	15.563610
27.692643	1409.325724	15.568627
27.711332	1405.689155	15.573645
27.857995	1396.627381	15.578663
27.550403	1401.481949	15.583680
27.870974	1403.068321	15.588698
27.625322	1410.760125	15.593715
27.611751	1394.810616	15.598733
27.614769	1401.454465	15.603751
27.987385	1415.975107	15.608768
28.267861	1424.462302	15.613786
28.176091	1424.190676	15.618803
27.655339	1413.004843	15.623821
28.083706	1432.396030	15.628839
27.833991	1425.437635	15.633856
27.842200	1422.993489	15.638874
28.167474	1445.603750	15.643891
28.381551	1432.309283	15.648909
28.153934	1433.481312	15.653927
28.135768	1428.162794	15.658944
28.294279	1426.852397	15.663962
28.380084	1432.896329	15.668979
28.808939	1423.402572	15.673997
28.664878	1421.583597	15.679015
28.422221	1418.616335	15.684032
28.632788	1411.864523	15.689050
28.545648	1402.129046	15.694067
28.607855	1390.077909	15.699085
28.650714	1387.760373	15.704103
28.187507	1399.531027	15.709120
28.224263	1396.668636	15.714138
28.161373	1410.160790	15.719155
28.735105	1418.587049	15.724173
28.527148	1421.788246	15.729191
28.328183	1426.054500	15.734208
28.753239	1424.764508	15.739226
28.581620	1426.759717	15.744243
28.319841	1425.840394	15.749261
28.889163	1421.365677	15.754279
28.793286	1424.868315	15.759296
28.608636	1423.353110	15.764314
28.471105	1433.670308	15.769331
28.589172	1431.221223	15.774349
28.679331	1422.100807	15.779367
28.489407	1431.026397	15.784384
28.682614	1422.429081	15.789402
28.486094	1432.779283	15.794419
28.849330	1428.471139	15.799437
29.127977	1412.806901	15.804455
28.910972	1448.076588	15.809472
29.026957	1423.080538	15.814490
29.163173	1418.835348	15.819507
28.949511	1445.366526	15.824525
29.028828	1412.288006	15.829543
28.927096	1432.004412	15.834560
29.132659	1440.177955	15.839578
29.404290	1441.265634	15.844595
29.258531	1431.003096	15.849613
29.177185	1418.606752	15.854631
28.950211	1422.473213	15.859648
29.222632	1430.930236	15.864666
29.520654	1447.105013	15.869683
29.466171	1434.396064	15.874701
29.371065	1436.728275	15.879719
29.046349	1440.599320	15.884736
29.364194	1432.858276	15.889754
29.600458	1445.920510	15.894771
29.500346	1446.048182	15.899789
29.475289	1435.259884	15.904807
29.250013	1429.209926	15.909824
29.511687	1434.368526	15.914842
29.627172	1443.176198	15.919859
29.545378	1449.816295	15.924877
29.733225	1439.552449	15.929895
29.504670	1445.811692	15.934912
30.056095	1450.104552	15.939930
29.915549	1431.941601	15.944947
29.561749	1426.026972	15.949965
29.863227	1414.936500	15.954983
29.449581	1414.025671	15.960000
29.524911	1409.017857	15.965018
29.646724	1419.252781	15.970035
29.886072	1436.209244	15.975053
29.716641	1439.783392	15.980071
29.359854	1443.289899	15.985088
29.757002	1439.006230	15.990106
29.854843	1452.516830	15.995123
29.713295	1446.887655	16.000141
30.228839	1430.889890	16.005159
29.982545	1434.654045	16.010176
29.864355	1443.812015	16.015194
30.018858	1452.248534	16.020211
29.752223	1458.682168	16.025229
30.100355	1439.322862	16.030247
29.664526	1446.321441	16.035264
30.012506	1439.431296	16.040282
30.139004	1440.118988	16.045299
29.642511	1454.584816	16.050317
30.290718	1466.447232	16.055335
30.326651	1464.833919	16.060352
30.422313	1490.214743	16.065370
30.719406	1474.756706	16.070387
30.070811	1462.660011	16.075405
30.561523	1465.930673	16.080423
30.217112	1459.248483	16.085440
30.219911	1468.673456	16.090458
30.607214	1482.982615	16.095475
30.689024	1487.738921	16.100493
30.732496	1457.568199	16.105511
30.758862	1445.971037	16.110528
30.480233	1447.322659	16.115546
30.459742	1455.318340	16.120563
30.439643	1449.257668	16.125581
30.691195	1461.189640	16.130599
30.761948	1474.132010	16.135616
30.533535	1455.696758	16.140634
30.869835	1455.492131	16.145651
30.590651	1473.593117	16.150669
30.871372	1469.479017	16.155687
30.678022	1475.023236	16.160704
30.715321	1488.472741	16.165722
31.088859	1477.133207	16.170739
30.912527	1475.248587	16.175757
31.032584	1485.697766	16.180775
30.910036	1474.533313	16.185792
30.806256	1476.544449	16.190810
31.129098	1482.045662	16.195827
30.757459	1476.228238	16.200845
30.875600	1481.013353	16.205863
30.664746	1482.480008	16.210880
30.607470	1472.777472	16.215898
30.925619	1482.940228	16.220915
30.797769	1476.136973	16.225933
30.809435	1470.903342	16.230951
31.147673	1476.331312	16.235968
31.163806	1497.373921	16.240986
31.356123	1495.026238	16.246003
31.044584	1492.387693	16.251021
31.210706	1480.772930	16.256039
31.368975	1493.297097	16.261056
31.632924	1502.359547	16.266074
31.633408	1482.245538	16.271091
31.214648	1474.389158	16.276109
31.686349	1469.752249	16.281127
31.160905	1484.013514	16.286144
31.219582	1479.760225	16.291162
31.335488	1500.171882	16.296179
31.432204	1499.478513	16.301197
31.621213	1496.023965	16.306215
31.417779	1500.934310	16.311232
31.668806	1509.992533	16.316250
31.706054	1480.684761	16.321267
31.327670	1519.354443	16.326285
31.657271	1485.241698	16.331303
31.637705	1521.209942	16.336320
31.744624	1472.013046	16.341338
31.876764	1508.216605	16.346355
31.356363	1503.819723	16.351373
32.043899	1479.361613	16.356391
31.903465	1508.758242	16.361408
32.044816	1467.362680	16.366426
31.730569	1495.750401	16.371443
31.286849	1500.008525	16.376461
31.927313	1486.899252	16.381479
32.216988	1536.537918	16.386496
32.154064	1515.809494	16.391514
32.519035	1519.902457	16.396531
31.968849	1511.675341	16.401549
32.164990	1488.848147	16.406567
32.278628	1490.667307	16.411584
32.077256	1512.034062	16.416602
32.365145	1479.928841	16.421619
31.908595	1514.639157	16.426637
32.327233	1494.941347	16.431655
32.236962	1531.557959	16.436672
32.514434	1526.252025	16.441690
32.505633	1521.432194	16.446707
32.633869	1528.057702	16.451725
32.578050	1506.356042	16.456743
32.454606	1508.785591	16.461760
32.284657	1487.435639	16.466778
32.164305	1496.196018	16.471795
31.869135	1536.066829	16.476813
32.196149	1497.309385	16.481831
32.340644	1530.704797	16.486848
32.215095	1515.517046	16.491866
32.617656	1529.971680	16.496883
32.576618	1512.799478	16.501901
32.492575	1536.307287	16.506919
33.006446	1524.084898	16.511936
32.928740	1523.306093	16.516954
32.708336	1524.550909	16.521971
32.497600	1534.401662	16.526989
33.241308	1525.203681	16.532007
32.918508	1529.829485	16.537024
32.710990	1533.579615	16.542042
32.782368	1528.443403	16.547059
32.715443	1546.822079	16.552077
33.300888	1554.666112	16.557095
33.161724	1565.000967	16.562112
33.146499	1541.763815	16.567130
33.452775	1543.000131	16.572147
33.383520	1536.758502	16.577165
33.332689	1507.497757	16.582183
33.405890	1503.270459	16.587200
33.211095	1507.325288	16.592218
33.547866	1501.522274	16.597235
33.108519	1508.936716	16.602253
33.279540	1521.724712	16.607271
33.476946	1512.895442	16.612288
33.077179	1509.297277	16.617306
33.085036	1515.954564	16.622323
33.359963	1512.060024	16.627341
33.424436	1516.161591	16.632359
33.458856	1515.616582	16.637376
33.240149	1511.841675	16.642394
33.541996	1528.355702	16.647411
33.679660	1545.177503	16.652429
33.684923	1539.853634	16.657447
33.668504	1525.768446	16.662464
33.615623	1538.779357	16.667482
34.031196	1531.077729	16.672499
33.573414	1515.016470	16.677517
33.579614	1519.287778	16.682535
33.765092	1532.204037	16.687552
33.853419	1531.985479	16.692570
33.867577	1529.095206	16.697587
33.787369	1540.672752	16.702605
33.700030	1539.801102	16.707623
33.789423	1536.743100	16.712640
34.161159	1537.937515	16.717658
34.177182	1535.893220	16.722675
33.812709	1541.235099	16.727693
33.901085	1543.390199	16.732711
33.963563	1544.394844	16.737728
33.828601	1543.467869	16.742746
34.440610	1530.654103	16.747763
34.461988	1540.079305	16.752781
34.080799	1536.478170	16.757799
34.192690	1533.602195	16.762816
33.786951	1539.048182	16.767834
34.201065	1533.558431	16.772851
34.077264	1538.973606	16.777869
34.248927	1533.656231	16.782887
34.422759	1538.517425	16.787904
33.945145	1525.577015	16.792922
34.089438	1540.922276	16.797939
34.389427	1532.104946	16.802957
34.519161	1567.063217	16.807975
34.656008	1572.885138	16.812992
34.828379	1568.944021	16.818010
34.946427	1543.277333	16.823027
34.448115	1539.664992	16.828045
34.077323	1536.221072	16.833063
34.459299	1547.603784	16.838080
34.756729	1563.470477	16.843098
34.686376	1563.786883	16.848115
34.631763	1570.853703	16.853133
34.543326	1563.076720	16.858151
34.582402	1564.045774	16.863168
34.857321	1573.631903	16.868186
35.015328	1569.424092	16.873203
34.889610	1560.608580	16.878221
34.859308	1576.124870	16.883239
35.116093	1569.126516	16.888256
34.767766	1573.256188	16.893274
34.847315	1571.650063	16.898291
34.659049	1580.496830	16.903309
35.020143	1575.789441	16.908327
35.047378	1566.548411	16.913344
34.545157	1577.424096	16.918362
35.120665	1585.650400	16.923379
35.247851	1586.528324	16.928397
34.860935	1595.273078	16.933415
35.131431	1589.529363	16.938432
34.840197	1594.052625	16.943450
35.255679	1584.046523	16.948467
35.284514	1585.846188	16.953485
35.086536	1582.480085	16.958503
35.350553	1600.017965	16.963520
35.383916	1620.660033	16.968538
35.972383	1599.465799	16.973555
35.635068	1599.145245	16.978573
35.662168	1597.453103	16.983591
36.139710	1575.425597	16.988608
35.724589	1574.271175	16.993626
35.645127	1589.611278	16.998643
35.695460	1571.077936	17.003661
35.340286	1590.474763	17.008679
35.885018	1579.243122	17.013696
35.671341	1608.230068	17.018714
36.251618	1595.775234	17.023731
36.020354	1588.986847	17.028749
35.826485	1584.289321	17.033767
36.143203	1591.745232	17.038784
36.037652	1576.849953	17.043802
35.924276	1575.035502	17.048819
35.896482	1575.736800	17.053837
36.017035	1589.113345	17.058855
36.179535	1560.965191	17.063872
36.146785	1593.654425	17.068890
36.034189	1596.777529	17.073907
36.228047	1598.226834	17.078925
36.112863	1600.375085	17.083943
36.316551	1588.153355	17.088960
36.214869	1612.681838	17.093978
36.191183	1610.831055	17.098995
36.122088	1616.583596	17.104013
35.970280	1622.818089	17.109031
36.308645	1617.057247	17.114048
36.090422	1611.317543	17.119066
36.043761	1610.006822	17.124083
36.247375	1602.793565	17.129101
36.354206	1617.378825	17.134119
36.546444	1615.163269	17.139136
36.608828	1630.999886	17.144154
36.796410	1627.270257	17.149171
36.890350	1617.326429	17.154189
36.880933	1622.006096	17.159207
36.861449	1597.876061	17.164224
36.409841	1623.850919	17.169242
37.050117	1617.184629	17.174259
36.713752	1603.181857	17.179277
36.629337	1632.146660	17.184295
36.865896	1625.200269	17.189312
36.698189	1638.386885	17.194330
36.966141	1641.400539	17.199347
37.150172	1636.933729	17.204365
36.889247	1638.365914	17.209383
37.336116	1628.546683	17.214400
37.645391	1638.717257	17.219418
37.633319	1635.179918	17.224435
37.847413	1616.986911	17.229453
37.461596	1616.710271	17.234471
37.539338	1598.263758	17.239488
37.452255	1605.567007	17.244506
37.489110	1602.558269	17.249523
37.472612	1598.383002	17.254541
37.380204	1602.739275	17.259559
37.494327	1607.503052	17.264576
37.101620	1617.667601	17.269594
37.329684	1595.440758	17.274611
37.257137	1592.960701	17.279629
37.021607	1613.441155	17.284647
37.225002	1588.201219	17.289664
37.058307	1621.885574	17.294682
37.357713	1628.648994	17.299699
37.612726	1616.997922	17.304717
37.362235	1625.875090	17.309735
37.673112	1632.394437	17.314752
37.916868	1631.680756	17.319770
37.599572	1631.621275	17.324787
37.963944	1610.942537	17.329805
37.570951	1637.449186	17.334823
38.002826	1608.737306	17.339840
37.806687	1641.745289	17.344858
37.946596	1618.454956	17.349875
38.002367	1618.609675	17.354893
37.869425	1639.094252	17.359911
38.267783	1641.583741	17.364928
37.996586	1623.081167	17.369946
38.086032	1654.218931	17.374963
38.722453	1653.406440	17.379981
38.423757	1631.280864	17.384999
38.282605	1621.365092	17.390016
38.183225	1630.164678	17.395034
38.251587	1616.138238	17.400051
38.399317	1616.492220	17.405069
38.014804	1617.909508	17.410087
38.491736	1648.224117	17.415104
38.582025	1648.709957	17.420122
38.954523	1648.770115	17.425139
38.661710	1620.176945	17.430157
38.410727	1629.796656	17.435175
38.479174	1621.761813	17.440192
38.585020	1636.617809	17.445210
38.639572	1661.874931	17.450227
38.852245	1651.957759	17.455245
38.886657	1658.771324	17.460263
38.943360	1652.619667	17.465280
38.951469	1636.863060	17.470298
38.646210	1624.681576	17.475315
38.601078	1623.499597	17.480333
38.442360	1646.319503	17.485351
38.779582	1664.331848	17.490368
38.605803	1649.996359	17.495386
38.844311	1644.998616	17.500403
38.904121	1661.065338	17.505421
38.563140	1655.272837	17.510439
38.719378	1661.096420	17.515456
39.063010	1662.054656	17.520474
39.109330	1704.680874	17.525491
39.422681	1681.754459	17.530509
39.017662	1686.085112	17.535527
39.041180	1680.029972	17.540544
39.280872	1692.822896	17.545562
38.984065	1691.088024	17.550579
39.468841	1677.699821	17.555597
38.902729	1684.989852	17.560615
39.187221	1666.621960	17.565632
39.653099	1691.659372	17.570650
39.760805	1697.580373	17.575667
39.708587	1681.432219	17.580685
39.745957	1684.987599	17.585703
39.699477	1684.625374	17.590720
39.857249	1673.438078	17.595738
39.713105	1679.070480	17.600755
39.703472	1671.836146	17.605773
39.604380	1685.093657	17.610791
39.970592	1692.234988	17.615808
40.413292	1700.989055	17.620826
40.163686	1692.605353	17.625843
40.236720	1671.501091	17.630861
40.081362	1670.866796	17.635879
40.123923	1667.781630	17.640896
40.442564	1671.115967	17.645914
40.032536	1667.119851	17.650931
40.180376	1674.654651	17.655949
40.189686	1681.558746	17.660967
40.006500	1670.457295	17.665984
40.326638	1660.507247	17.671002
39.803546	1677.270997	17.676019
40.237453	1672.419831	17.681037
39.664452	1673.005173	17.686055
40.211532	1697.411447	17.691072
40.231579	1703.959911	17.696090
40.170696	1709.506685	17.701107
40.330283	1710.259899	17.706125
40.481222	1697.187620	17.711143
40.558265	1699.385450	17.716160
40.758878	1695.505861	17.721178
40.408788	1714.522943	17.726195
40.863202	1689.618747	17.731213
40.706632	1704.283860	17.736231
40.428297	1710.052507	17.741248
40.545550	1683.147729	17.746266
40.591469	1699.455808	17.751283
40.615714	1699.643871	17.756301
40.907966	1724.602069	17.761319
40.995640	1735.172997	17.766336
41.096858	1726.445457	17.771354
40.884768	1726.087623	17.776371
41.055151	1722.724082	17.781389
41.175285	1734.296569	17.786407
41.346889	1725.411511	17.791424
41.571493	1731.694553	17.796442
41.038562	1709.503970	17.801459
41.379086	1707.835756	17.806477
41.173739	1722.964844	17.811495
41.591590	1719.192173	17.816512
41.334815	1702.082470	17.821530
41.034204	1726.913435	17.826547
41.407535	1726.945147	17.831565
41.569805	1717.515743	17.836583
41.327740	1714.837759	17.841600
41.531926	1728.801991	17.846618
41.246402	1735.668194	17.851635
41.509114	1706.243780	17.856653
41.530034	1738.397817	17.861671
41.674795	1718.776421	17.866688
42.034903	1729.055355	17.871706
41.681245	1736.336694	17.876723
41.808734	1717.182098	17.881741
41.686750	1722.282445	17.886759
41.999388	1726.149435	17.891776
42.220408	1723.177366	17.896794
41.804703	1721.653362	17.901811
41.979587	1709.023992	17.906829
41.610337	1743.602953	17.911847
41.889360	1717.617700	17.916864
42.070501	1735.900420	17.921882
42.021187	1716.572677	17.926899
41.907500	1728.685822	17.931917
42.210962	1753.801157	17.936935
42.396347	1750.965327	17.941952
42.312787	1752.926085	17.946970
42.272908	1752.352020	17.951987
42.560644	1753.559852	17.957005
42.566607	1758.191492	17.962023
42.355386	1752.842298	17.967040
42.848822	1749.608123	17.972058
42.576414	1751.284396	17.977075
42.642906	1725.406959	17.982093
42.471688	1718.198374	17.987111
42.390856	1735.610524	17.992128
42.708378	1745.543904	17.997146
42.589129	1742.825877	18.002163
42.681387	1762.365500	18.007181
42.607404	1754.710378	18.012199
42.259778	1754.075285	18.017216
42.707027	1758.397441	18.022234
42.363108	1752.144471	18.027251
42.583302	1750.424659	18.032269
42.585453	1746.144128	18.037287
42.707245	1782.134518	18.042304
42.750200	1768.662545	18.047322
42.586103	1808.192297	18.052339
43.185333	1760.946688	18.057357
43.013613	1787.545733	18.062375
43.169302	1781.969693	18.067392
43.192110	1765.976219	18.072410
43.110916	1810.863082	18.077427
43.353797	1807.819869	18.082445
43.781216	1796.904077	18.087463
43.370992	1791.964137	18.092480
43.300028	1806.662890	18.097498
43.590446	1800.138837	18.102515
43.601664	1818.842023	18.107533
43.995213	1788.252979	18.112551
43.543882	1817.443415	18.117568
43.950768	1793.573815	18.122586
43.703110	1798.140526	18.127603
43.970608	1794.519232	18.132621
44.185204	1775.581902	18.137639
44.156564	1777.562218	18.142656
44.101161	1739.307144	18.147674
43.838155	1778.143157	18.152691
44.187677	1753.062100	18.157709
43.969456	1764.433747	18.162727
43.784325	1780.752028	18.167744
44.097503	1755.656313	18.172762
44.308167	1770.827638	18.177779
44.177743	1755.664007	18.182797
43.873413	1759.190535	18.187815
44.036183	1757.575836	18.192832
44.153343	1749.177648	18.197850
43.847190	1783.619225	18.202867
44.286062	1777.386111	18.207885
44.366066	1779.995615	18.212903
44.262654	1794.897734	18.217920
44.393730	1800.911004	18.222938
44.363138	1792.385346	18.227955
44.328589	1778.837635	18.232973
44.101901	1794.470425	18.237991
44.284594	1798.166250	18.243008
44.241081	1792.080855	18.248026
44.396537	1805.220798	18.253043
44.407955	1833.412515	18.258061
44.741227	1818.266097	18.263079
44.527282	1828.054638	18.268096
44.697182	1818.085974	18.273114
44.658015	1822.551798	18.278131
44.729227	1826.243389	18.283149
45.077267	1822.994636	18.288167
44.897202	1823.065849	18.293184
45.319443	1829.795615	18.298202
45.179680	1831.228942	18.303219
45.425620	1819.882752	18.308237
45.270177	1808.352050	18.313255
45.033976	1823.707962	18.318272
45.337004	1842.147556	18.323290
45.653745	1837.363788	18.328307
45.272025	1825.947815	18.333325
45.077161	1844.768847	18.338343
45.551094	1842.948779	18.343360
45.595146	1830.263092	18.348378
45.604839	1842.709013	18.353395
45.921005	1846.141314	18.358413
46.201420	1830.300166	18.363431
45.375917	1822.959928	18.368448
45.714486	1812.031556	18.373466
45.680308	1818.730293	18.378483
46.093275	1819.930742	18.383501
45.756994	1818.003946	18.388519
45.758556	1824.409121	18.393536
46.045360	1841.729728	18.398554
46.027636	1836.961552	18.403571
46.077225	1833.024217	18.408589
46.305871	1829.523943	18.413607
45.576603	1840.391990	18.418624
45.778414	1838.379368	18.423642
45.922933	1836.268919	18.428659
46.178868	1836.711042	18.433677
46.180150	1833.747257	18.438695
46.105518	1835.640534	18.443712
46.175158	1836.820238	18.448730
46.330424	1841.682923	18.453747
46.472926	1835.284694	18.458765
46.566908	1826.511057	18.463783
46.552193	1844.112567	18.468800
46.365284	1825.173143	18.473818
46.658331	1831.811830	18.478835
46.245656	1840.364208	18.483853
46.517142	1847.846344	18.488871
46.347415	1848.162875	18.493888
46.927679	1848.038886	18.498906
46.642101	1856.193473	18.503923
46.820807	1862.263668	18.508941
46.845667	1857.848920	18.513959
46.671887	1863.081848	18.518976
46.883109	1856.606581	18.523994
47.016217	1854.648961	18.529011
46.922079	1846.927791	18.534029
47.225938	1851.875320	18.539047
47.092716	1854.410306	18.544064
47.282404	1854.858277	18.549082
47.333672	1848.377066	18.554099
47.073195	1855.220453	18.559117
47.498112	1849.337176	18.564135
46.993180	1855.680001	18.569152
46.965445	1868.528319	18.574170
47.389543	1877.351529	18.579187
47.596076	1890.222278	18.584205
47.789573	1880.004413	18.589223
47.656971	1884.046280	18.594240
47.663732	1878.901375	18.599258
47.690129	1884.399688	18.604275
47.502329	1887.616647	18.609293
48.028354	1880.325089	18.614311
48.158302	1888.054766	18.619328
47.916204	1868.271498	18.624346
48.132965	1879.111383	18.629363
47.972630	1890.900191	18.634381
48.479206	1880.029916	18.639399
48.062942	1869.530208	18.644416
48.133624	1861.787461	18.649434
47.767253	1854.034201	18.654451
47.939708	1867.129017	18.659469
48.349984	1885.881901	18.664487
48.435587	1876.341925	18.669504
48.418362	1884.282265	18.674522
48.344553	1883.702594	18.679539
48.123203	1880.222170	18.684557
48.428958	1874.955645	18.689575
48.053258	1875.215365	18.694592
48.368006	1877.133061	18.699610
48.321415	1880.605925	18.704627
48.289432	1881.529704	18.709645
48.677633	1862.736033	18.714663
48.408965	1877.088860	18.719680
48.687095	1889.199421	18.724698
48.626963	1893.602544	18.729715
48.735077	1903.813255	18.734733
49.205804	1901.974815	18.739751
48.742389	1918.845728	18.744768
48.940933	1904.655099	18.749786
49.029149	1903.396772	18.754803
49.012861	1907.468859	18.759821
49.189093	1907.498975	18.764839
49.078336	1904.147199	18.769856
49.059961	1908.933781	18.774874
49.245555	1911.916583	18.779891
49.068458	1907.482121	18.784909
49.479413	1899.507328	18.789927
49.037191	1909.970989	18.794944
49.293481	1909.884515	18.799962
49.373482	1902.712849	18.804979
49.041141	1909.492217	18.809997
49.192269	1912.060513	18.815015
49.551437	1926.244039	18.820032
49.365193	1935.668006	18.825050
49.915614	1942.835139	18.830067
49.953686	1936.764985	18.835085
49.800529	1926.657433	18.840103
49.683462	1927.969171	18.845120
49.900069	1935.375161	18.850138
50.154704	1934.126469	18.855155
50.174526	1932.449606	18.860173
50.045325	1920.318444	18.865191
50.184399	1932.584929	18.870208
50.468419	1932.105490	18.875226
50.412453	1926.523826	18.880243
49.986023	1914.279625	18.885261
50.212236	1929.165488	18.890279
50.313045	1927.189414	18.895296
49.933609	1925.755558	18.900314
50.113511	1928.795901	18.905331
50.057126	1927.521309	18.910349
50.355752	1926.945158	18.915367
50.223967	1933.417266	18.920384
50.507026	1940.515354	18.925402
50.549578	1923.983721	18.930419
50.560090	1936.413861	18.935437
50.588386	1945.155521	18.940455
50.555565	1938.778917	18.945472
50.606331	1941.629071	18.950490
50.894748	1944.280871	18.955507
50.738811	1943.280135	18.960525
50.833797	1937.886753	18.965543
50.909808	1940.432428	18.970560
51.029944	1933.655473	18.975578
51.185703	1930.435792	18.980595
51.077257	1946.836410	18.985613
51.299829	1936.639037	18.990631
51.066880	1937.259813	18.995648
50.784660	1958.673152	19.000666
51.049842	1958.583687	19.005683
51.319011	1957.351552	19.010701
51.471202	1960.761269	19.015719
51.579464	1969.527943	19.020736
51.572190	1962.390616	19.025754
51.650148	1957.091180	19.030771
51.787280	1966.182015	19.035789
51.970492	1951.970189	19.040807
51.861994	1972.122569	19.045824
52.014426	1964.151221	19.050842
51.909923	1950.095400	19.055859
51.423284	1977.658962	19.060877
52.040075	1947.932190	19.065895
52.076123	1962.066612	19.070912
52.048211	1967.836318	19.075930
52.450652	1964.207619	19.080947
52.101087	1955.452735	19.085965
52.134729	1967.111564	19.090983
52.187187	1964.951284	19.096000
51.924183	1965.814386	19.101018
52.196374	1963.677263	19.106035
52.176340	1972.201701	19.111053
52.604346	1957.991726	19.116071
52.288998	1961.044997	19.121088
52.053801	1951.603329	19.126106
52.150257	1966.017561	19.131123
52.078938	1970.232151	19.136141
52.598586	1987.319165	19.141159
52.830899	1989.297216	19.146176
52.506306	1989.220017	19.151194
52.756154	1982.991796	19.156211
52.599667	1996.285487	19.161229
52.633127	1986.187456	19.166247
52.563766	1988.658796	19.171264
52.738613	1983.450865	19.176282
52.708961	1977.168122	19.181299
52.846835	2013.291805	19.186317
53.313802	2004.930488	19.191335
53.286722	2016.784662	19.196352
53.296670	2036.189914	19.201370
53.348479	2010.531393	19.206387
53.314594	2038.817253	19.211405
53.450032	2000.288803	19.216423
53.591998	2030.214039	19.221440
53.288702	2015.002201	19.226458
53.513914	1993.467351	19.231475
53.503047	2038.288643	19.236493
53.615238	2009.277743	19.241511
53.657803	2020.883281	19.246528
53.701188	2023.901373	19.251546
54.231257	2008.072126	19.256563
53.941288	2015.511760	19.261581
53.923901	2004.109897	19.266599
53.957645	2015.616162	19.271616
54.013268	2016.005295	19.276634
54.061250	2015.730244	19.281651
54.204551	2010.582392	19.286669
54.130352	2006.916442	19.291687
54.169765	2006.161403	19.296704
53.973969	2011.685764	19.301722
54.166761	2001.324778	19.306739
53.788594	2011.418065	19.311757
54.047793	2006.937582	19.316775
54.206395	2011.656645	19.321792
54.131205	2016.837723	19.326810
54.677676	2027.573223	19.331827
54.580418	2034.362346	19.336845
54.585070	2033.638019	19.341863
54.898842	2015.024340	19.346880
54.679542	2042.694827	19.351898
54.959146	2020.765862	19.356915
54.593975	2044.215508	19.361933
54.840279	2031.121427	19.366951
54.824955	2019.042808	19.371968
54.848535	2036.155514	19.376986
54.876581	2042.828700	19.382003
54.515965	2039.792029	19.387021
54.881362	2032.318371	19.392039
55.156651	2032.842361	19.397056
55.104644	2046.965740	19.402074
55.153115	2050.846636	19.407091
55.238148	2069.107353	19.412109
55.490972	2058.376521	19.417127
55.468879	2057.777583	19.422144
55.010552	2066.906822	19.427162
55.390820	2061.387668	19.432179
55.587206	2063.947201	19.437197
55.474746	2053.372162	19.442215
55.760664	2051.259580	19.447232
55.472177	2068.687944	19.452250
55.694752	2054.825253	19.457267
55.651473	2065.516412	19.462285
55.691450	2068.804050	19.467303
55.707546	2089.910447	19.472320
55.730242	2088.777388	19.477338
56.017286	2077.613211	19.482355
55.655070	2099.030076	19.487373
56.021049	2088.232410	19.492391
56.129484	2079.604183	19.497408
55.895557	2089.037426	19.502426
56.258190	2107.791905	19.507443
56.527230	2104.322878	19.512461
56.664451	2107.167141	19.517479
57.031749	2106.616212	19.522496
56.905843	2098.050518	19.527514
56.828163	2091.089530	19.532531
56.593938	2086.281869	19.537549
56.542106	2074.432401	19.542567
56.840070	2065.088099	19.547584
56.590866	2084.201258	19.552602
56.620136	2092.692734	19.557619
56.892472	2097.695715	19.562637
56.988680	2105.146164	19.567655
57.145578	2098.987776	19.572672
56.714952	2101.636307	19.577690
56.738459	2112.740004	19.582707
57.164302	2084.691984	19.587725
57.055737	2111.059746	19.592743
57.333673	2092.890569	19.597760
57.495304	2093.026838	19.602778
57.518573	2080.007612	19.607795
57.483852	2102.215411	19.612813
57.317565	2082.608527	19.617831
57.303355	2104.341139	19.622848
57.382828	2099.200289	19.627866
57.645845	2092.617555	19.632883
57.588594	2108.565013	19.637901
57.704340	2114.568276	19.642919
57.743611	2138.512008	19.647936
57.830808	2121.667854	19.652954
57.950716	2128.710257	19.657971
58.020404	2132.274750	19.662989
58.147502	2130.873346	19.668007
58.302422	2117.919607	19.673024
58.256226	2151.392483	19.678042
58.361928	2122.424865	19.683059
58.311347	2119.695815	19.688077
58.145817	2120.974399	19.693095
58.628595	2125.410555	19.698112
58.163899	2145.398183	19.703130
58.141528	2125.633003	19.708147
58.321451	2123.763838	19.713165
58.399467	2124.503343	19.718183
58.158131	2121.897527	19.723200
57.987991	2149.747572	19.728218
58.463645	2127.028959	19.733235
58.462908	2178.538545	19.738253
58.201894	2154.333632	19.743271
58.779333	2153.673678	19.748288
59.045624	2186.205650	19.753306
59.312012	2185.538674	19.758323
59.303676	2175.112899	19.763341
59.251220	2183.794434	19.768359
59.364527	2144.529000	19.773376
59.169490	2179.496500	19.778394
59.582406	2142.891334	19.783411
59.571645	2166.743202	19.788429
59.140310	2148.418870	19.793447
59.275489	2167.826348	19.798464
59.268899	2189.031678	19.803482
59.376434	2165.857320	19.808499
59.669312	2197.281566	19.813517
59.416872	2183.339565	19.818535
59.789870	2172.941065	19.823552
59.642155	2174.156249	19.828570
59.897452	2164.588233	19.833587
60.149138	2165.388920	19.838605
59.810882	2184.761814	19.843623
60.095914	2168.091340	19.848640
59.990906	2157.237389	19.853658
59.930903	2182.249412	19.858675
60.015923	2172.378203	19.863693
59.776717	2177.557968	19.868711
60.355542	2185.826566	19.873728
59.693648	2205.892919	19.878746
60.239221	2218.024811	19.883763
60.229111	2201.717560	19.888781
60.464526	2207.585367	19.893799
60.579168	2183.437686	19.898816
60.412902	2222.552046	19.903834
60.777115	2193.639015	19.908851
60.886340	2202.183086	19.913869
60.859114	2213.032247	19.918887
61.016954	2194.436131	19.923904
60.975786	2203.151271	19.928922
60.812957	2195.436151	19.933939
60.930733	2215.507160	19.938957
61.109895	2208.675044	19.943975
61.146982	2231.032828	19.948992
61.466393	2223.485395	19.954010
61.253910	2215.104119	19.959027
61.322435	2232.673947	19.964045
61.513519	2227.366596	19.969063
61.569185	2211.781111	19.974080
61.363034	2226.858152	19.979098
61.347931	2235.254538	19.984115
61.562410	2212.862174	19.989133
61.217956	2214.686845	19.994151
61.552695	2213.296363	19.999168
61.669436	2220.247290	20.004186
61.865294	2218.724009	20.009203
62.296393	2230.480113	20.014221
62.051221	2226.330912	20.019239
62.158518	2229.227164	20.024256
62.062236	2214.943251	20.029274
62.145243	2220.366594	20.034291
62.135086	2235.959030	20.039309
62.069558	2244.855839	20.044327
62.415281	2236.619912	20.049344
62.306544	2246.104079	20.054362
62.424110	2251.805863	20.059379
62.460935	2243.955838	20.064397
62.395348	2248.046894	20.069415
62.744439	2231.035784	20.074432
62.775862	2247.287014	20.079450
62.612943	2238.480166	20.084467
62.885842	2234.080016	20.089485
62.605690	2249.875196	20.094503
62.771192	2234.361835	20.099520
62.600676	2239.515723	20.104538
62.914530	2253.858601	20.109555
63.248938	2256.649422	20.114573
63.044370	2263.202500	20.119591
63.293453	2282.647023	20.124608
63.227874	2259.791933	20.129626
63.306550	2274.227397	20.134643
63.480380	2265.685375	20.139661
63.221470	2265.207572	20.144679
63.393409	2263.202805	20.149696
63.111174	2267.462131	20.154714
63.401589	2261.008664	20.159731
63.414444	2258.872748	20.164749
63.331507	2263.541537	20.169767
63.409707	2275.025187	20.174784
63.320669	2295.060075	20.179802
63.639786	2290.415001	20.184819
63.808722	2289.288491	20.189837
63.968832	2300.309981	20.194855
63.933663	2301.158787	20.199872
63.738517	2293.435397	20.204890
64.239951	2287.999872	20.209907
64.455267	2318.211317	20.214925
64.284801	2308.594702	20.219943
64.481041	2332.207753	20.224960
64.915679	2289.646965	20.229978
64.856480	2320.783125	20.234995
64.665982	2288.875119	20.240013
64.945073	2303.256626	20.245031
64.403541	2290.273805	20.250048
64.914622	2291.038636	20.255066
65.007336	2298.895599	20.260083
65.194561	2304.340106	20.265101
64.795964	2308.611710	20.270119
65.087414	2287.129572	20.275136
64.894081	2323.176283	20.280154
64.948167	2307.538249	20.285171
64.940652	2306.885064	20.290189
65.050889	2293.088829	20.295207
64.913358	2313.143275	20.300224
65.295276	2305.166602	20.305242
65.288263	2296.408003	20.310259
65.591183	2299.172393	20.315277
65.257396	2336.237301	20.320295
65.907690	2324.401496	20.325312
65.798474	2318.692102	20.330330
65.581924	2331.152501	20.335347
66.123033	2331.722202	20.340365
66.044991	2328.972322	20.345383
65.949132	2326.285848	20.350400
65.607525	2323.780147	20.355418
65.928980	2336.411946	20.360435
66.161551	2313.551694	20.365453
65.827444	2331.511486	20.370471
65.719914	2328.144938	20.375488
66.101660	2326.554245	20.380506
65.757194	2338.172998	20.385523
65.999893	2356.280723	20.390541
66.136417	2352.850864	20.395559
66.134231	2341.675983	20.400576
66.249400	2357.135298	20.405594
66.562911	2383.031165	20.410611
66.920183	2389.144679	20.415629
67.237568	2387.137149	20.420647
67.275878	2372.143385	20.425664
67.070606	2350.371485	20.430682
66.805027	2369.781798	20.435699
67.020094	2362.426335	20.440717
66.870976	2375.548516	20.445735
67.303844	2373.633473	20.450752
67.143155	2376.129669	20.455770
67.206523	2378.258994	20.460787
67.591991	2380.829329	20.465805
67.402907	2385.948474	20.470823
67.460640	2383.149401	20.475840
67.396744	2379.777455	20.480858
67.510483	2386.387580	20.485875
67.508732	2367.207121	20.490893
67.517058	2368.261361	20.495911
67.466132	2378.291696	20.500928
67.751297	2396.946430	20.505946
67.759832	2406.253902	20.510963
68.253421	2398.038349	20.515981
68.441184	2402.674235	20.520999
68.389156	2405.804369	20.526016
68.400496	2397.395943	20.531034
68.102109	2397.952450	20.536051
68.310443	2387.336230	20.541069
68.470243	2390.267402	20.546087
68.355517	2399.022706	20.551104
68.641772	2387.872577	20.556122
68.630553	2396.503614	20.561139
68.799167	2389.754111	20.566157
68.962058	2401.470544	20.571175
68.596812	2399.265915	20.576192
68.992812	2383.436409	20.581210
68.667451	2390.582202	20.586227
68.852653	2385.632825	20.591245
68.833277	2398.053969	20.596263
69.197209	2397.758411	20.601280
69.076488	2419.270943	20.606298
68.857844	2425.101138	20.611315
69.065107	2416.107722	20.616333
68.977820	2416.345045	20.621351
69.001613	2422.122416	20.626368
68.838531	2424.568663	20.631386
69.113928	2437.215761	20.636403
69.500222	2436.096263	20.641421
69.555434	2444.464251	20.646439
69.910004	2447.337629	20.651456
70.032746	2447.655505	20.656474
69.574772	2439.032453	20.661491
70.107906	2446.816109	20.666509
69.710366	2458.032841	20.671527
69.718978	2456.205900	20.676544
70.044140	2459.564554	20.681562
70.080514	2464.645410	20.686579
70.323135	2469.416508	20.691597
70.562245	2477.060660	20.696615
70.381614	2479.158911	20.701632
70.534317	2465.914193	20.706650
70.388302	2468.207493	20.711667
70.700765	2465.100350	20.716685
70.860100	2471.190409	20.721703
70.641526	2478.134374	20.726720
70.834809	2462.169578	20.731738
70.826638	2462.509120	20.736755
70.719247	2467.494923	20.741773
70.894404	2476.544619	20.746791
70.889497	2482.958980	20.751808
71.443623	2477.307334	20.756826
70.926212	2498.744029	20.761843
71.417448	2494.111555	20.766861
71.407162	2502.553734	20.771879
71.290747	2505.296161	20.776896
71.403726	2493.474339	20.781914
71.611171	2503.800200	20.786931
71.696211	2495.133771	20.791949
71.672176	2497.473692	20.796967
71.582720	2485.077729	20.801984
71.601929	2507.596100	20.807002
71.719361	2513.513525	20.812019
71.797383	2513.032316	20.817037
71.905814	2535.037038	20.822055
72.020196	2523.539029	20.827072
72.653512	2519.115135	20.832090
72.199494	2520.398075	20.837107
72.033732	2519.554602	20.842125
71.988041	2526.546527	20.847143
72.155702	2532.266388	20.852160
72.036723	2536.443123	20.857178
72.402870	2557.292225	20.862195
72.985324	2541.785191	20.867213
72.838757	2543.687672	20.872231
72.647508	2552.074578	20.877248
73.277151	2545.875216	20.882266
73.215523	2537.837803	20.887283
73.272079	2535.600489	20.892301
73.267255	2536.991125	20.897319
73.089475	2545.783317	20.902336
73.355538	2530.961504	20.907354
72.906192	2537.407443	20.912371
73.178287	2539.155059	20.917389
73.370277	2538.622638	20.922407
73.026210	2538.589438	20.927424
73.677726	2529.859388	20.932442
73.545165	2564.406479	20.937459
73.909567	2564.644917	20.942477
73.804671	2557.276675	20.947495
73.886882	2562.693194	20.952512
74.057926	2571.859229	20.957530
73.991664	2565.945461	20.962547
74.104302	2559.541454	20.967565
74.304575	2562.376539	20.972583
74.117553	2566.804820	20.977600
74.432931	2550.724495	20.982618
74.408408	2556.251635	20.987635
74.528518	2563.012629	20.992653
74.609435	2560.596024	20.997671
74.529694	2549.393238	21.002688
74.841738	2555.506958	21.007706
75.005666	2563.215059	21.012723
74.639780	2558.281936	21.017741
74.709771	2562.624393	21.022759
74.557084	2570.124215	21.027776
74.974249	2549.188752	21.032794
74.823016	2554.483614	21.037811
74.869117	2575.435699	21.042829
74.995011	2568.535614	21.047847
74.753142	2583.830304	21.052864
74.989961	2583.939643	21.057882
74.835785	2590.020760	21.062899
75.008058	2592.430855	21.067917
75.315574	2601.734029	21.072935
75.281887	2618.696883	21.077952
75.472907	2620.861732	21.082970
75.756454	2610.164925	21.087987
75.680477	2615.295214	21.093005
75.719604	2613.757561	21.098023
75.682439	2628.644461	21.103040
76.214147	2638.626889	21.108058
76.364523	2648.506536	21.113075
76.300951	2650.757613	21.118093
76.492141	2635.526038	21.123111
76.523359	2637.403324	21.128128
76.553828	2631.843785	21.133146
76.582463	2641.306300	21.138163
76.866778	2639.243446	21.143181
77.095906	2635.094779	21.148199
76.783477	2628.737295	21.153216
77.251953	2621.894242	21.158234
76.901649	2632.519158	21.163251
77.083546	2631.370892	21.168269
77.530356	2619.402127	21.173287
77.155110	2613.946628	21.178304
77.152405	2606.005179	21.183322
77.510145	2618.800549	21.188339
77.100444	2623.922713	21.193357
77.489993	2624.028145	21.198375
76.832201	2625.505623	21.203392
77.182682	2615.016015	21.208410
77.133972	2626.580748	21.213427
77.005896	2627.394836	21.218445
77.059021	2630.358801	21.223463
77.217536	2651.171149	21.228480
77.566772	2633.999090	21.233498
77.637014	2664.900611	21.238515
78.130557	2642.119355	21.243533
77.987832	2677.369948	21.248551
77.933771	2655.414588	21.253568
78.080812	2672.799382	21.258586
78.292374	2680.577032	21.263603
78.253220	2656.848737	21.268621
78.344892	2677.318616	21.273639
78.459171	2688.022859	21.278656
78.612526	2656.662501	21.283674
78.777507	2666.455669	21.288691
78.931514	2667.164993	21.293709
79.022089	2668.485368	21.298727
78.658955	2669.159182	21.303744
79.079447	2675.034633	21.308762
79.294803	2691.758853	21.313779
79.006462	2706.442055	21.318797
79.438536	2695.995223	21.323815
79.459228	2701.577346	21.328832
79.526506	2685.548239	21.333850
79.475830	2687.847605	21.338867
79.115352	2707.758025	21.343885
79.254141	2676.429838	21.348903
79.274121	2702.679849	21.353920
79.668793	2699.931593	21.358938
79.668730	2706.350786	21.363955
79.693424	2732.805393	21.368973
80.099452	2696.936165	21.373991
80.056705	2734.971125	21.379008
80.227782	2714.715725	21.384026
80.394811	2703.043999	21.389043
80.300954	2729.139955	21.394061
80.535319	2696.251665	21.399079
80.449131	2718.075330	21.404096
80.431530	2706.990722	21.409114
80.308723	2713.283979	21.414131
80.172644	2704.179178	21.419149
80.695620	2733.540910	21.424167
80.629678	2744.277870	21.429184
80.719287	2732.369913	21.434202
80.792150	2734.817123	21.439219
80.700543	2759.952377	21.444237
81.190085	2724.883859	21.449255
81.214274	2757.001873	21.454272
81.532126	2756.789170	21.459290
81.392193	2765.766594	21.464307
81.358003	2773.695179	21.469325
81.499354	2750.730805	21.474343
81.449586	2766.346645	21.479360
81.734210	2760.158171	21.484378
81.741751	2748.935805	21.489395
81.606090	2769.804678	21.494413
82.173601	2742.718375	21.499431
81.842277	2760.073377	21.504448
81.638216	2760.917681	21.509466
82.051026	2757.634015	21.514483
81.865530	2760.957769	21.519501
82.094770	2795.833127	21.524519
82.284367	2791.599478	21.529536
82.471976	2792.827306	21.534554
82.452976	2776.516108	21.539571
82.109533	2797.539289	21.544589
82.880474	2789.140852	21.549607
82.485256	2784.536396	21.554624
83.157183	2819.640107	21.559642
83.243339	2797.050219	21.564659
82.645364	2814.370727	21.569677
83.084551	2807.857900	21.574695
82.951295	2809.164431	21.579712
83.104568	2828.134932	21.584730
83.036282	2809.363294	21.589747
82.910167	2809.645357	21.594765
83.457455	2815.657172	21.599783
83.625154	2837.258827	21.604800
83.911422	2845.728634	21.609818
84.176270	2841.351613	21.614835
83.829922	2843.506233	21.619853
84.402086	2841.219681	21.624871
84.171793	2842.621133	21.629888
84.272816	2818.321191	21.634906
84.134946	2809.475391	21.639923
84.232365	2829.815571	21.644941
84.488975	2829.349919	21.649959
84.356985	2839.756897	21.654976
84.443492	2842.348252	21.659994
84.326760	2836.982011	21.665011
84.429161	2841.203756	21.670029
84.563809	2833.298484	21.675047
84.658639	2836.747449	21.680064
84.561301	2839.952547	21.685082
84.807364	2853.020785	21.690099
84.853464	2865.409861	21.695117
85.268722	2853.534821	21.700135
84.966359	2856.384839	21.705152
84.966493	2882.097175	21.710170
85.509262	2860.685023	21.715187
85.301882	2875.120296	21.720205
85.409721	2864.982264	21.725223
85.407882	2871.644078	21.730240
85.449611	2875.963606	21.735258
85.799255	2901.060982	21.740275
85.524517	2900.009904	21.745293
85.923879	2876.714725	21.750311
86.009016	2891.178875	21.755328
85.933942	2912.074471	21.760346
86.163813	2887.234725	21.765363
86.099255	2888.523227	21.770381
86.200331	2895.978812	21.775399
85.861140	2912.994663	21.780416
86.451741	2917.070141	21.785434
86.661243	2903.502124	21.790451
86.583903	2925.382107	21.795469
86.931048	2897.947599	21.800487
86.775370	2896.488178	21.805504
86.924442	2925.504843	21.810522
86.857386	2909.763563	21.815539
86.891593	2916.909687	21.820557
86.935649	2917.704205	21.825575
87.338980	2934.929667	21.830592
87.419410	2935.712879	21.835610
87.698213	2940.812659	21.840627
87.498905	2951.582839	21.845645
87.938257	2941.172429	21.850663
87.949556	2938.949351	21.855680
87.773921	2943.236704	21.860698
87.871971	2939.361348	21.865715
87.934972	2942.064232	21.870733
87.683757	2951.891716	21.875751
87.996535	2939.800909	21.880768
87.896695	2918.630379	21.885786
87.655210	2934.532611	21.890803
87.862633	2948.605264	21.895821
88.353136	2950.078982	21.900839
88.432090	2960.446111	21.905856
88.295292	2967.110614	21.910874
88.369638	2953.846487	21.915891
88.315230	2981.387055	21.920909
88.620545	2998.971174	21.925927
88.589152	2985.517797	21.930944
88.836272	3003.117495	21.935962
89.019198	2978.394415	21.940979
89.164169	2996.487850	21.945997
89.310549	3003.874126	21.951015
89.197535	3012.458835	21.956032
89.880599	3002.579788	21.961050
90.084230	3013.834001	21.966067
90.006462	3005.748561	21.971085
89.976479	3008.523706	21.976103
90.182227	3017.795398	21.981120
90.011130	3005.407291	21.986138
90.030637	2994.419589	21.991155
90.042500	3001.138271	21.996173
89.988700	3011.838095	22.001191
90.186499	3001.316714	22.006208
89.991328	3013.159963	22.011226
90.494207	3013.036525	22.016243
90.412372	3007.439693	22.021261
90.439778	3015.095868	22.026279
90.665817	3011.990597	22.031296
90.386966	3022.053004	22.036314
90.782868	3023.614182	22.041331
90.792674	3038.345344	22.046349
91.181376	3042.246186	22.051367
91.338230	3044.787817	22.056384
91.025178	3038.096739	22.061402
91.067504	3039.066160	22.066419
91.101473	3029.432983	22.071437
91.234550	3028.815551	22.076455
91.164368	3044.744858	22.081472
91.429423	3035.177866	22.086490
91.734044	3069.743743	22.091507
91.533907	3054.822701	22.096525
91.468399	3062.445737	22.101543
91.771640	3067.266361	22.106560
91.498678	3052.483575	22.111578
91.891639	3080.546069	22.116595
92.059490	3086.017559	22.121613
92.160196	3084.245073	22.126631
92.264353	3107.857552	22.131648
92.017412	3084.258448	22.136666
92.491123	3116.097119	22.141683
92.135057	3120.698043	22.146701
92.337650	3132.305692	22.151719
92.223827	3112.724446	22.156736
92.512841	3131.757074	22.161754
92.857982	3136.770046	22.166771
92.769739	3159.246779	22.171789
93.160214	3138.429574	22.176807
93.806970	3133.390608	22.181824
93.614576	3148.364934	22.186842
93.654272	3125.158182	22.191859
93.313694	3124.654039	22.196877
93.664915	3154.743292	22.201895
94.572164	3121.147356	22.206912
93.834845	3160.945243	22.211930
94.262865	3135.899638	22.216947
94.427805	3118.847648	22.221965
94.623488	3136.031738	22.226983
94.570075	3109.408759	22.232000
94.327831	3139.910406	22.237018
94.592571	3123.484351	22.242035
94.553666	3128.756000	22.247053
94.216815	3127.500071	22.252071
94.394216	3125.854576	22.257088
94.468715	3150.323728	22.262106
94.495669	3150.094486	22.267123
94.978878	3156.536705	22.272141
95.223313	3151.285013	22.277159
94.963107	3149.000585	22.282176
95.024328	3149.506846	22.287194
95.423498	3158.382805	22.292211
95.467451	3175.256051	22.297229
95.465405	3169.987026	22.302247
95.775441	3173.099700	22.307264
95.504761	3184.233825	22.312282
95.712843	3169.165759	22.317299
95.699020	3173.168586	22.322317
95.596238	3173.589306	22.327335
95.817860	3175.966459	22.332352
96.047822	3184.074174	22.337370
96.279903	3182.850218	22.342387
96.100898	3194.675303	22.347405
96.503834	3210.096714	22.352423
96.778974	3198.735363	22.357440
96.563752	3198.086158	22.362458
96.557576	3191.727566	22.367475
96.482865	3212.066626	22.372493
96.495108	3203.515218	22.377511
96.631999	3199.576964	22.382528
96.881729	3192.430299	22.387546
97.205557	3230.977586	22.392563
97.344817	3230.798080	22.397581
97.223082	3228.095900	22.402599
97.511581	3229.558600	22.407616
97.417277	3231.827253	22.412634
97.389663	3227.337080	22.417651
97.728700	3219.576775	22.422669
97.888682	3230.859356	22.427687
98.045848	3213.347550	22.432704
97.796916	3224.586788	22.437722
98.326164	3243.334261	22.442739
98.329455	3247.121998	22.447757
98.128488	3248.137312	22.452775
98.416398	3237.024818	22.457792
98.237289	3244.106797	22.462810
98.579437	3245.104718	22.467827
98.435454	3252.844199	22.472845
98.974715	3242.954889	22.477863
99.064494	3243.053076	22.482880
98.604620	3249.395596	22.487898
98.786884	3264.879787	22.492915
98.969739	3264.775135	22.497933
99.029648	3270.946675	22.502951
99.148859	3272.982274	22.507968
99.310669	3276.601579	22.512986
99.513277	3275.958105	22.518003
99.385245	3286.467025	22.523021
99.588043	3301.456358	22.528039
99.682129	3296.253763	22.533056
99.756809	3303.310242	22.538074
99.809738	3306.587443	22.543091
99.995686	3300.574160	22.548109
99.907000	3313.919590	22.553127
100.429109	3328.801394	22.558144
100.441302	3347.268049	22.563162
100.312374	3348.112202	22.568179
100.473017	3322.886310	22.573197
100.244100	3340.528507	22.578215
100.768944	3337.799495	22.583232
100.725232	3344.229863	22.588250
100.901617	3346.585154	22.593267
101.379352	3354.010012	22.598285
100.949723	3372.068117	22.603303
101.304429	3355.275058	22.608320
100.970180	3379.440077	22.613338
101.248209	3352.695364	22.618355
101.328331	3346.610052	22.623373
101.603868	3372.623864	22.628391
101.819192	3351.496051	22.633408
101.546324	3369.600735	22.638426
102.074634	3375.098231	22.643443
101.923499	3383.871729	22.648461
102.201866	3386.007034	22.653479
102.140713	3372.328358	22.658496
102.338181	3396.624140	22.663514
102.166392	3390.156577	22.668531
102.226540	3387.395471	22.673549
102.214831	3394.317890	22.678567
102.867309	3403.944926	22.683584
102.655651	3416.248933	22.688602
102.702330	3398.382462	22.693619
103.041322	3417.652128	22.698637
102.965783	3407.401376	22.703655
103.127460	3408.778915	22.708672
103.503641	3423.136612	22.713690
103.547989	3440.641746	22.718707
103.880560	3431.682001	22.723725
103.705192	3426.960469	22.728743
104.287638	3428.821533	22.733760
104.339226	3430.458118	22.738778
103.985452	3435.211375	22.743795
104.332061	3424.576288	22.748813
104.526962	3429.499264	22.753831
104.489031	3428.393862	22.758848
104.515151	3430.656713	22.763866
104.550136	3414.589479	22.768883
105.103295	3422.867610	22.773901
104.567850	3440.813670	22.778919
105.076790	3402.203076	22.783936
105.081577	3440.463556	22.788954
104.926378	3413.752422	22.793971
104.842959	3421.561780	22.798989
104.510910	3432.583168	22.804007
104.940655	3422.118891	22.809024
104.867426	3434.083048	22.814042
104.960965	3439.511461	22.819059
105.119398	3439.685228	22.824077
105.081227	3459.760798	22.829095
105.275089	3476.057503	22.834112
105.527932	3469.117085	22.839130
105.680371	3477.149227	22.844147
106.006389	3485.473056	22.849165
105.967509	3496.825312	22.854183
106.257791	3496.841184	22.859200
106.200606	3510.212448	22.864218
106.396700	3502.310389	22.869235
106.460676	3498.650345	22.874253
106.361713	3495.721872	22.879271
106.819271	3516.603401	22.884288
106.583470	3499.348214	22.889306
106.672103	3510.988497	22.894323
106.981212	3521.668578	22.899341
106.979538	3551.348468	22.904359
107.277110	3523.178921	22.909376
107.103422	3536.722963	22.914394
107.126900	3533.192866	22.919411
107.598475	3515.697423	22.924429
107.531966	3541.969816	22.929447
107.899282	3541.610776	22.934464
107.627858	3545.263052	22.939482
107.619909	3547.713848	22.944499
108.340035	3539.385240	22.949517
108.209004	3547.077186	22.954535
108.170146	3540.025931	22.959552
108.327365	3562.864525	22.964570
108.610163	3577.901954	22.969587
109.119551	3565.577908	22.974605
108.379106	3569.577152	22.979623
108.529540	3564.732825	22.984640
108.578935	3568.470816	22.989658
108.724573	3579.464908	22.994675
109.101660	3592.475160	22.999693
109.289144	3602.523380	23.004711
109.201701	3591.933792	23.009728
109.179468	3591.533826	23.014746
109.466090	3593.431862	23.019763
109.952383	3608.757023	23.024781
109.775851	3631.503424	23.029799
110.128274	3624.329949	23.034816
110.053452	3610.536024	23.039834
110.174187	3623.750014	23.044851
110.132227	3634.869244	23.049869
110.310549	3611.041786	23.054887
110.439581	3628.830982	23.059904
110.561920	3627.368054	23.064922
110.479508	3644.668675	23.069939
110.702791	3637.219233	23.074957
110.590637	3654.272104	23.079975
111.095029	3655.652438	23.084992
110.930209	3650.854422	23.090010
110.955094	3648.868201	23.095027
111.420205	3655.882256	23.100045
111.303752	3665.975054	23.105063
111.422389	3666.450153	23.110080
111.800836	3668.839351	23.115098
111.629279	3679.145467	23.120115
111.923656	3669.302004	23.125133
111.672880	3680.846305	23.130151
112.247191	3681.615302	23.135168
112.178493	3653.643145	23.140186
111.753074	3689.761700	23.145203
112.198610	3684.801052	23.150221
112.339638	3702.787438	23.155239
112.212955	3698.988625	23.160256
111.969266	3702.241633	23.165274
112.538694	3717.761320	23.170291
113.113467	3715.388485	23.175309
112.856572	3731.300330	23.180327
113.113603	3740.080533	23.185344
113.640584	3725.621805	23.190362
113.305372	3724.255431	23.195379
113.667618	3715.684094	23.200397
113.327665	3720.275552	23.205415
113.488459	3719.338239	23.210432
113.615685	3744.766736	23.215450
113.774426	3749.388805	23.220467
113.939326	3745.903754	23.225485
114.031696	3753.114168	23.230503
114.158575	3750.902427	23.235520
114.522620	3744.507369	23.240538
114.433801	3742.119212	23.245555
114.276053	3748.645031	23.250573
114.291618	3774.251856	23.255591
114.809286	3778.808045	23.260608
115.072314	3774.834578	23.265626
114.832539	3768.476016	23.270643
115.156658	3767.467031	23.275661
115.070633	3781.663589	23.280679
115.415363	3793.516552	23.285696
115.729301	3789.563281	23.290714
115.408199	3797.428047	23.295731
115.623951	3796.503204	23.300749
115.631556	3802.330115	23.305767
115.685034	3793.762347	23.310784
115.653724	3813.236326	23.315802
116.176152	3819.162857	23.320819
116.497003	3820.659793	23.325837
116.420520	3831.421257	23.330855
116.598833	3830.888616	23.335872
116.876312	3814.823178	23.340890
116.792835	3815.360404	23.345907
117.324275	3805.189570	23.350925
117.378218	3822.862756	23.355943
117.128720	3815.307692	23.360960
116.932866	3814.654582	23.365978
116.830206	3824.662694	23.370995
117.462852	3832.609016	23.376013
117.516335	3847.305711	23.381031
117.450645	3845.387398	23.386048
117.649082	3846.207693	23.391066
117.877636	3847.937246	23.396083
117.757835	3842.275350	23.401101
117.438024	3854.299624	23.406119
118.211951	3861.289706	23.411136
118.300107	3874.890633	23.416154
118.333878	3880.262664	23.421171
118.677884	3873.628465	23.426189
118.429245	3872.116904	23.431207
118.226999	3876.246725	23.436224
118.571043	3890.374807	23.441242
118.473191	3897.994783	23.446259
118.825364	3904.707597	23.451277
118.929597	3908.645388	23.456295
119.128579	3917.217059	23.461312
119.494510	3927.581591	23.466330
119.358503	3935.449166	23.471347
119.348352	3928.986266	23.476365
119.351133	3926.201169	23.481383
119.644912	3947.908652	23.486400
120.053990	3943.115778	23.491418
120.042756	3952.990617	23.496435
120.641274	3948.984845	23.501453
120.537993	3937.883860	23.506471
120.463625	3940.538038	23.511488
120.762566	3939.731289	23.516506
120.510277	3946.192821	23.521523
120.530473	3954.987323	23.526541
120.918432	3963.825447	23.531559
120.803303	3975.575684	23.536576
120.865539	3977.011615	23.541594
121.103138	3982.191493	23.546611
121.160879	3991.663615	23.551629
121.200223	4002.065334	23.556647
121.368913	4005.099254	23.561664
121.395243	4004.601070	23.566682
121.685570	4025.421893	23.571699
121.786471	4033.188025	23.576717
122.402698	4045.229170	23.581735
122.232662	4040.962051	23.586752
122.422312	4024.488753	23.591770
122.649056	4033.872595	23.596787
123.005279	4029.567971	23.601805
122.501725	4044.398529	23.606823
122.876702	4061.893375	23.611840
123.311080	4040.827182	23.616858
123.162446	4054.348040	23.621875
123.536633	4053.445903	23.626893
123.420633	4051.813268	23.631911
123.413372	4050.770578	23.636928
123.802490	4055.415793	23.641946
123.675163	4048.899941	23.646963
123.678325	4050.436549	23.651981
123.736430	4061.808390	23.656999
123.668449	4074.378732	23.662016
123.879979	4073.748749	23.667034
123.849697	4083.091012	23.672051
124.234216	4093.481018	23.677069
124.572818	4109.756923	23.682087
124.418340	4107.634047	23.687104
124.943880	4113.798557	23.692122
124.770741	4117.904138	23.697139
125.052269	4114.099905	23.702157
124.617298	4120.539513	23.707175
124.801508	4131.910965	23.712192
125.349573	4133.343384	23.717210
125.103792	4139.730019	23.722227
125.115721	4131.656397	23.727245
125.617704	4147.796161	23.732263
125.667641	4159.298390	23.737280
126.042295	4169.947256	23.742298
126.034055	4176.510781	23.747315
126.253400	4176.294111	23.752333
126.464420	4167.869344	23.757351
126.321152	4172.028388	23.762368
126.970587	4180.330936	23.767386
126.607078	4200.964427	23.772403
126.714093	4199.472422	23.777421
126.985106	4190.785562	23.782439
126.881713	4198.217781	23.787456
127.609569	4189.363676	23.792474
127.318706	4197.910573	23.797491
127.252002	4192.621598	23.802509
127.268916	4201.491502	23.807527
127.219831	4225.847645	23.812544
127.858500	4221.073925	23.817562
127.428265	4212.973222	23.822579
127.988951	4232.044992	23.827597
128.405830	4248.542204	23.832615
128.280324	4250.283426	23.837632
128.573651	4245.762216	23.842650
128.558551	4241.898267	23.847667
128.663788	4244.326411	23.852685
128.910401	4253.019695	23.857703
128.605478	4259.592808	23.862720
129.041172	4261.058106	23.867738
129.127391	4275.156090	23.872755
129.022142	4267.025561	23.877773
129.515694	4280.040671	23.882791
129.075630	4301.521932	23.887808
129.344506	4300.980341	23.892826
129.736408	4291.636958	23.897843
129.687069	4299.229738	23.902861
129.996862	4315.084888	23.907879
129.898462	4329.645809	23.912896
130.280754	4312.819728	23.917914
130.332149	4327.012993	23.922931
130.603341	4343.788420	23.927949
130.925365	4347.238488	23.932967
130.682379	4353.048151	23.937984
131.292221	4356.457046	23.943002
131.207941	4356.972392	23.948019
131.362728	4351.696026	23.953037
131.279758	4347.777581	23.958055
131.138238	4359.080006	23.963072
131.528839	4361.514584	23.968090
131.488947	4373.165822	23.973107
131.672325	4382.139090	23.978125
131.876066	4389.655375	23.983143
131.658875	4382.100371	23.988160
131.705878	4396.826183	23.993178
132.050797	4402.337588	23.998195
132.425288	4405.913035	24.003213
132.810569	4393.142392	24.008231
132.437394	4419.822400	24.013248
132.847229	4429.867200	24.018266
133.049882	4436.584438	24.023283
132.648070	4441.735856	24.028301
133.297019	4441.025095	24.033319
133.123388	4444.632889	24.038336
133.473838	4465.041196	24.043354
133.373505	4480.078504	24.048371
133.464133	4470.352745	24.053389
133.560290	4473.072653	24.058407
133.409998	4487.863843	24.063424
133.592711	4510.096481	24.068442
133.938249	4502.428083	24.073459
133.946214	4521.185597	24.078477
134.486439	4519.857333	24.083495
134.579405	4535.988016	24.088512
135.094753	4523.362507	24.093530
134.743329	4542.799606	24.098547
134.865884	4534.921309	24.103565
135.382173	4553.943154	24.108583
135.017703	4564.973702	24.113600
135.639952	4555.738954	24.118618
135.318283	4568.062251	24.123635
135.183976	4572.103551	24.128653
135.786553	4569.404409	24.133671
135.674135	4584.376097	24.138688
135.996762	4600.405723	24.143706
136.389073	4608.847066	24.148723
136.555959	4608.520756	24.153741
136.754941	4596.312218	24.158759
136.780461	4609.294481	24.163776
137.001893	4596.143869	24.168794
137.324634	4607.105774	24.173811
137.217112	4625.682023	24.178829
137.362192	4628.999107	24.183847
137.630452	4631.867028	24.188864
137.428487	4631.850481	24.193882
137.739722	4640.650119	24.198899
137.744075	4631.808068	24.203917
138.150855	4624.458669	24.208935
137.922502	4642.373738	24.213952
138.092225	4642.652710	24.218970
138.506029	4655.285964	24.223987
138.392349	4668.491864	24.229005
138.997254	4657.386755	24.234023
138.801210	4656.970422	24.239040
138.726074	4658.322911	24.244058
138.694559	4651.155096	24.249075
138.855521	4654.910189	24.254093
138.920228	4675.889063	24.259111
138.861856	4691.039469	24.264128
138.849755	4693.653173	24.269146
139.259908	4700.797648	24.274163
139.267424	4707.986664	24.279181
139.430792	4708.097516	24.284199
139.696959	4731.291085	24.289216
139.838234	4737.928567	24.294234
140.212338	4740.900781	24.299251
140.130964	4744.353909	24.304269
140.815109	4749.169427	24.309287
140.699198	4765.753754	24.314304
140.627641	4762.907191	24.319322
140.988196	4772.936486	24.324339
141.021944	4773.453479	24.329357
141.266471	4775.544831	24.334375
141.219748	4790.191581	24.339392
141.607195	4786.427717	24.344410
141.620267	4793.774011	24.349427
141.674548	4810.954299	24.354445
141.773630	4803.126803	24.359463
141.975659	4815.711363	24.364480
141.987266	4824.053055	24.369498
142.272239	4819.986130	24.374515
142.020057	4839.697294	24.379533
142.704553	4845.221588	24.384551
142.860824	4851.191986	24.389568
142.846138	4854.046854	24.394586
142.863133	4852.999453	24.399603
142.989547	4879.708405	24.404621
143.569568	4876.941219	24.409639
143.618997	4883.099376	24.414656
143.801430	4867.806311	24.419674
144.028203	4861.280835	24.424691
144.049881	4866.612675	24.429709
144.260117	4886.367381	24.434727
144.250179	4905.303670	24.439744
144.602302	4910.974603	24.444762
144.706294	4911.636165	24.449779
144.384881	4916.188058	24.454797
144.796500	4901.538895	24.459815
144.840452	4898.847744	24.464832
145.442563	4907.946516	24.469850
145.568357	4918.449169	24.474867
145.373946	4920.443755	24.479885
145.697607	4914.119931	24.484903
145.634282	4911.045461	24.489920
145.717224	4914.202594	24.494938
145.962927	4916.975048	24.499955
145.928092	4924.633493	24.504973
146.223025	4932.439964	24.509991
146.562276	4956.397907	24.515008
146.353703	4957.796874	24.520026
147.002250	4943.098878	24.525043
146.780723	4955.549705	24.530061
146.768610	4947.156141	24.535079
146.806761	4958.154249	24.540096
147.060470	4959.824072	24.545114
147.400753	4978.546487	24.550131
147.245164	4984.189843	24.555149
147.412116	4976.436395	24.560167
147.511095	4983.470931	24.565184
147.347446	5002.551431	24.570202
147.974491	5011.865780	24.575219
147.891396	5020.369794	24.580237
148.096198	5037.343834	24.585255
148.198882	5036.315011	24.590272
148.327921	5037.006412	24.595290
148.340566	5046.226011	24.600307
148.218251	5067.602651	24.605325
148.831692	5063.234690	24.610343
148.820430	5079.277173	24.615360
149.107918	5087.347670	24.620378
149.566420	5093.563412	24.625395
149.925334	5091.419105	24.630413
150.095082	5088.008490	24.635431
149.852664	5094.128308	24.640448
150.446442	5107.314624	24.645466
151.028194	5115.449140	24.650483
150.820663	5115.259618	24.655501
151.027952	5106.421897	24.660519
151.425165	5107.505583	24.665536
151.086627	5117.154117	24.670554
151.272257	5106.832996	24.675571
151.052670	5112.658105	24.680589
151.367567	5113.509467	24.685607
151.532884	5118.041241	24.690624
151.337694	5110.175540	24.695642
151.639920	5115.526459	24.700659
151.445486	5140.816712	24.705677
151.825833	5136.831259	24.710695
151.864759	5133.182670	24.715712
151.513601	5153.374971	24.720730
151.910796	5159.389682	24.725747
152.341405	5178.480285	24.730765
152.870262	5195.719878	24.735783
152.827230	5202.320090	24.740800
152.988358	5186.251259	24.745818
153.238678	5197.974094	24.750835
153.003121	5224.316571	24.755853
153.202096	5224.405231	24.760871
153.778916	5226.557736	24.765888
153.467662	5231.608446	24.770906
153.924263	5235.827906	24.775923
153.853882	5242.213007	24.780941
154.322585	5251.374963	24.785959
154.071547	5255.841788	24.790976
154.386383	5270.273237	24.795994
155.079261	5270.548264	24.801011
154.843682	5282.218050	24.806029
154.984005	5278.072581	24.811047
155.290088	5280.043266	24.816064
155.129418	5279.894258	24.821082
155.419594	5274.114514	24.826099
155.573071	5289.242769	24.831117
155.685008	5310.957668	24.836135
155.820427	5305.668317	24.841152
155.909291	5314.562823	24.846170
156.206304	5313.128523	24.851187
155.975188	5337.633537	24.856205
156.317779	5336.970807	24.861223
156.447266	5343.121113	24.866240
156.360907	5344.311031	24.871258
156.950856	5351.095170	24.876275
157.136703	5364.959610	24.881293
156.920028	5359.006543	24.886311
157.358216	5367.865835	24.891328
157.211511	5384.532865	24.896346
157.483877	5380.017015	24.901363
157.675081	5405.368172	24.906381
157.639776	5412.509290	24.911399
158.246430	5420.943677	24.916416
157.867002	5428.813884	24.921434
157.986210	5444.415857	24.926451
158.430450	5456.361299	24.931469
158.447208	5453.225170	24.936487
158.750391	5475.528960	24.941504
158.492182	5481.048045	24.946522
159.052186	5487.887372	24.951539
159.054045	5512.226506	24.956557
159.391207	5513.676182	24.961575
160.252971	5512.932239	24.966592
160.146033	5506.093867	24.971610
160.567142	5523.695608	24.976627
160.667783	5530.679004	24.981645
160.733218	5529.749706	24.986663
160.521930	5536.452421	24.991680
160.656761	5539.411817	24.996698
161.177472	5534.744608	25.001715
160.945172	5534.078344	25.006733
161.140052	5537.941544	25.011751
161.445684	5555.317853	25.016768
161.229263	5568.572408	25.021786
161.291870	5564.575354	25.026803
161.928389	5589.043141	25.031821
162.214901	5593.738257	25.036839
162.089049	5594.728372	25.041856
162.034580	5595.375109	25.046874
162.346832	5594.150768	25.051891
162.262478	5615.574858	25.056909
162.120134	5618.275577	25.061927
162.713798	5620.694517	25.066944
162.952185	5651.754112	25.071962
162.876377	5647.978146	25.076979
163.242509	5647.203871	25.081997
163.434676	5646.607598	25.087015
163.579229	5665.471453	25.092032
163.894046	5683.643401	25.097050
164.128209	5679.449816	25.102067
163.971037	5682.560435	25.107085
164.285999	5683.362260	25.112103
164.292756	5695.380013	25.117120
164.368302	5710.986870	25.122138
164.676491	5698.774172	25.127155
164.721524	5721.408225	25.132173
165.109324	5729.467803	25.137191
165.303483	5730.757783	25.142208
165.531071	5735.304994	25.147226
165.893815	5732.324482	25.152243
165.832950	5747.561337	25.157261
165.913454	5771.584682	25.162279
166.313771	5763.135907	25.167296
166.452208	5758.191289	25.172314
166.442821	5764.041354	25.177331
166.313540	5778.797444	25.182349
166.595214	5787.161919	25.187367
166.947112	5785.917868	25.192384
166.736095	5795.870641	25.197402
167.208211	5810.960429	25.202419
167.463160	5816.939089	25.207437
167.385738	5827.855572	25.212455
168.156294	5826.937345	25.217472
167.997031	5840.560661	25.222490
168.352539	5841.204191	25.227507
168.433123	5847.957277	25.232525
168.722453	5843.503881	25.237543
169.109810	5837.551865	25.242560
168.691457	5844.315269	25.247578
168.577546	5849.257621	25.252595
168.983934	5853.675659	25.257613
169.041521	5868.318649	25.262631
169.474823	5878.518842	25.267648
169.544763	5887.921796	25.272666
169.427453	5913.940606	25.277683
169.641637	5892.249964	25.282701
169.854822	5921.083747	25.287719
170.128277	5918.633536	25.292736
169.838693	5925.098726	25.297754
170.686946	5955.958660	25.302771
171.157938	5950.718638	25.307789
170.929157	5956.945993	25.312807
171.070663	5959.611743	25.317824
171.154988	5950.896189	25.322842
171.360259	5975.796069	25.327859
171.547934	5989.374432	25.332877
171.478788	5987.749056	25.337895
171.753398	5981.104532	25.342912
171.739035	6010.420852	25.347930
172.094497	6023.401319	25.352947
172.547553	6008.589471	25.357965
172.195605	6022.544212	25.362983
172.746313	6026.407453	25.368000
172.750695	6037.123802	25.373018
172.676367	6043.348595	25.378035
173.255406	6048.398457	25.383053
172.987095	6059.377803	25.388071
173.203837	6048.522373	25.393088
173.676931	6078.096260	25.398106
173.943060	6086.758415	25.403123
174.136078	6097.148914	25.408141
173.985482	6082.926530	25.413159
174.692206	6097.917054	25.418176
174.702666	6117.804398	25.423194
174.964564	6121.852968	25.428211
174.818038	6127.193201	25.433229
174.790906	6130.522350	25.438247
175.329428	6128.360278	25.443264
175.264263	6142.754830	25.448282
175.657295	6147.837531	25.453299
175.691208	6153.020763	25.458317
175.962447	6172.326891	25.463335
176.069111	6167.753042	25.468352
176.423774	6184.414201	25.473370
176.605229	6181.697746	25.478387
176.702071	6190.781116	25.483405
176.595961	6226.778648	25.488423
177.178700	6202.967493	25.493440
176.653294	6226.085074	25.498458
177.536211	6229.000076	25.503475
177.665578	6241.492019	25.508493
177.519428	6264.636521	25.513511
177.714327	6237.877804	25.518528
177.724669	6287.351344	25.523546
177.768752	6272.223650	25.528563
178.728262	6287.757052	25.533581
178.690466	6286.412237	25.538599
178.836567	6305.408839	25.543616
178.850558	6295.441549	25.548634
178.738185	6339.700529	25.553651
179.301530	6326.910064	25.558669
179.460548	6325.112162	25.563687
179.648556	6356.585668	25.568704
179.821442	6364.408430	25.573722
180.104139	6351.665050	25.578739
180.203683	6367.686545	25.583757
180.262188	6389.523270	25.588775
180.714704	6380.472606	25.593792
180.658156	6376.905808	25.598810
180.987433	6391.614572	25.603827
181.176288	6392.401143	25.608845
181.304402	6406.797393	25.613863
181.669275	6404.335675	25.618880
181.568432	6421.318346	25.623898
181.794162	6402.994043	25.628915
181.916883	6416.985980	25.633933
182.111418	6438.575288	25.638951
182.348149	6445.243956	25.643968
182.496235	6431.832764	25.648986
182.728645	6421.769197	25.654003
182.792364	6463.892730	25.659021
182.437895	6469.371666	25.664039
182.820676	6461.837157	25.669056
182.819735	6485.522176	25.674074
183.451173	6495.798997	25.679092
183.824674	6474.145831	25.684109
183.246816	6530.133201	25.689127
183.915860	6506.716134	25.694144
183.797340	6545.578686	25.699162
184.329244	6533.896111	25.704180
184.573424	6573.399560	25.709197
184.767443	6554.113970	25.714215
184.913837	6572.678932	25.719232
185.010508	6586.933244	25.724250
185.308627	6590.051711	25.729268
185.759381	6587.374071	25.734285
185.314019	6614.147430	25.739303
185.763035	6599.397795	25.744320
185.976310	6618.336097	25.749338
186.246793	6631.469909	25.754356
186.764502	6624.155347	25.759373
186.791198	6631.700224	25.764391
187.130576	6633.579244	25.769408
187.338010	6665.047163	25.774426
187.473296	6668.587357	25.779444
187.923260	6654.862689	25.784461
187.821231	6658.932453	25.789479
187.817486	6651.329658	25.794496
188.334017	6666.640623	25.799514
188.513612	6688.825910	25.804532
188.936547	6681.749088	25.809549
188.970124	6688.671343	25.814567
189.040670	6689.821402	25.819584
189.010153	6688.471456	25.824602
188.856950	6696.551734	25.829620
189.373905	6696.522836	25.834637
189.048327	6723.146687	25.839655
189.147458	6718.974342	25.844672
189.692024	6737.155807	25.849690
189.536629	6753.458335	25.854708
189.928764	6745.262082	25.859725
190.102026	6779.497297	25.864743
190.218197	6772.790350	25.869760
190.624676	6802.908964	25.874778
190.968304	6802.041450	25.879796
191.256242	6805.901165	25.884813
191.139765	6813.476043	25.889831
191.528034	6840.555138	25.894848
191.578165	6830.975907	25.899866
191.736202	6840.489733	25.904884
191.877206	6848.852851	25.909901
191.923324	6866.185537	25.914919
192.132611	6866.674618	25.919936
192.623148	6873.605143	25.924954
192.693193	6893.899453	25.929972
193.222209	6886.647478	25.934989
193.225985	6889.706722	25.940007
193.553545	6889.911799	25.945024
193.889751	6883.144544	25.950042
193.753445	6899.927277	25.955060
194.035808	6914.694398	25.960077
194.004874	6922.553100	25.965095
194.413483	6913.926902	25.970112
194.474679	6921.895228	25.975130
194.387575	6932.754271	25.980148
194.829873	6938.033961	25.985165
195.037443	6949.709934	25.990183
195.101640	6948.230778	25.995200
195.456572	6970.693021	26.000218
195.374555	6981.195658	26.005236
195.794862	6992.840894	26.010253
195.915765	6990.001767	26.015271
196.203374	6999.278669	26.020288
196.281961	7023.791380	26.025306
196.305715	7038.246583	26.030324
196.976852	7022.788406	26.035341
196.946366	7053.251003	26.040359
197.146537	7050.407881	26.045376
197.564589	7054.449125	26.050394
197.813076	7076.439111	26.055412
197.933293	7078.316939	26.060429
197.980973	7085.934235	26.065447
198.350102	7081.998056	26.070464
198.715013	7091.806371	26.075482
198.720151	7105.057656	26.080500
198.850896	7116.723192	26.085517
198.906590	7110.972257	26.090535
199.327834	7121.216153	26.095552
199.548736	7137.212052	26.100570
199.394193	7143.627911	26.105588
199.947837	7139.543492	26.110605
200.103768	7162.069226	26.115623
200.284863	7159.949837	26.120640
200.291338	7160.145527	26.125658
200.486715	7175.603429	26.130676
200.905510	7173.633401	26.135693
200.576709	7191.617131	26.140711
201.135969	7199.867343	26.145728
201.210640	7219.287220	26.150746
201.599203	7211.655424	26.155764
201.943688	7226.691483	26.160781
201.777601	7227.308876	26.165799
201.946021	7243.170057	26.170816
202.479367	7256.376605	26.175834
202.562709	7266.337720	26.180852
202.747492	7256.183620	26.185869
202.734628	7284.457340	26.190887
203.053566	7284.280623	26.195904
203.342325	7285.712238	26.200922
203.073010	7293.218096	26.205940
203.691365	7309.988769	26.210957
203.617113	7317.298310	26.215975
204.208484	7323.485172	26.220992
204.157047	7347.699702	26.226010
204.115954	7351.338207	26.231028
204.461036	7349.547501	26.236045
204.840092	7364.913371	26.241063
204.707748	7387.933105	26.246080
205.369058	7377.624268	26.251098
205.195213	7389.989276	26.256116
205.543971	7399.792504	26.261133
205.733356	7414.536394	26.266151
206.372887	7428.655399	26.271168
206.523176	7431.555277	26.276186
206.541509	7443.199651	26.281204
206.816594	7448.202473	26.286221
207.068005	7449.859581	26.291239
206.940792	7458.973156	26.296256
207.155707	7449.744929	26.301274
207.334174	7489.613793	26.306292
207.618958	7463.992806	26.311309
207.965882	7519.479244	26.316327
208.171890	7493.110696	26.321344
208.287479	7520.399742	26.326362
208.164074	7535.998540	26.331380
208.530900	7535.594663	26.336397
208.661038	7551.872214	26.341415
208.613937	7573.190904	26.346432
209.219015	7579.480339	26.351450
209.725799	7602.338710	26.356468
209.991661	7595.590218	26.361485
210.351064	7601.540366	26.366503
210.634262	7620.001426	26.371520
210.772183	7619.587619	26.376538
210.811652	7622.494973	26.381556
210.999648	7617.294774	26.386573
210.829762	7637.131077	26.391591
210.774107	7664.057421	26.396608
211.104173	7655.630585	26.401626
211.606162	7688.216651	26.406644
211.869255	7684.443572	26.411661
211.760272	7702.698950	26.416679
211.929606	7717.196125	26.421696
212.626183	7717.242460	26.426714
212.708171	7750.101771	26.431732
213.145208	7757.322146	26.436749
213.387405	7744.768155	26.441767
213.574410	7745.978415	26.446784
213.883896	7776.097950	26.451802
213.694462	7767.943501	26.456820
213.966188	7782.963400	26.461837
214.500970	7763.429930	26.466855
214.421841	7771.992327	26.471872
214.848922	7772.244503	26.476890
214.760578	7807.024223	26.481908
215.075816	7796.565697	26.486925
215.291400	7802.278411	26.491943
215.503430	7809.699920	26.496960
215.932436	7827.875977	26.501978
216.015721	7841.615103	26.506996
216.324957	7824.322237	26.512013
216.233396	7828.430780	26.517031
216.283744	7868.787683	26.522048
216.621478	7829.152645	26.527066
216.557128	7869.249294	26.532084
217.013396	7882.896341	26.537101
217.319700	7868.824830	26.542119
217.268105	7901.850945	26.547136
217.708055	7910.810642	26.552154
217.756254	7925.007874	26.557172
217.835965	7939.259895	26.562189
218.212189	7946.722179	26.567207
218.228209	7963.099418	26.572224
219.008888	7973.048191	26.577242
219.067991	7991.561964	26.582260
219.335936	8016.005207	26.587277
219.663390	8000.537084	26.592295
219.794527	8001.837318	26.597312
220.081394	8019.675894	26.602330
220.173702	8034.455548	26.607348
220.307383	8031.901387	26.612365
220.555114	8051.430887	26.617383
220.666482	8083.910136	26.622400
221.480728	8069.986826	26.627418
221.671923	8082.025895	26.632436
221.502213	8095.449144	26.637453
221.702592	8088.669168	26.642471
221.659055	8098.454355	26.647488
222.036652	8121.013087	26.652506
222.554156	8132.612256	26.657524
222.557607	8123.909897	26.662541
222.565727	8143.678365	26.667559
222.734539	8161.441510	26.672576
223.238769	8161.288755	26.677594
223.344058	8172.339136	26.682612
223.433028	8201.986380	26.687629
223.976518	8199.962511	26.692647
224.119613	8216.244231	26.697664
224.469844	8226.345994	26.702682
224.286243	8255.907753	26.707700
224.295456	8245.827396	26.712717
224.776780	8254.649302	26.717735
224.839721	8277.159289	26.722752
225.427850	8303.116244	26.727770
225.790785	8295.201568	26.732788
225.876844	8302.296400	26.737805
226.026014	8309.377239	26.742823
226.285688	8321.861180	26.747840
226.693372	8309.887007	26.752858
226.293145	8340.386001	26.757876
226.796937	8355.626789	26.762893
227.009273	8340.550430	26.767911
227.212702	8380.645107	26.772928
227.822518	8381.115243	26.777946
227.970876	8379.624104	26.782964
227.920950	8381.927380	26.787981
228.190551	8425.955415	26.792999
228.307312	8400.018108	26.798016
228.954852	8452.433016	26.803034
229.104286	8438.281719	26.808052
229.072239	8450.266971	26.813069
229.307622	8467.694104	26.818087
229.626626	8471.196789	26.823104
229.664487	8490.033251	26.828122
230.209859	8469.261783	26.833140
230.288803	8507.981522	26.838157
230.809133	8511.671660	26.843175
231.165905	8547.438920	26.848192
231.560955	8526.437176	26.853210
231.516874	8543.170858	26.858228
231.553397	8541.971365	26.863245
232.196076	8535.584934	26.868263
231.906179	8577.862108	26.873280
232.157850	8557.134193	26.878298
232.432976	8570.741115	26.883316
232.131626	8615.661772	26.888333
232.662594	8598.342895	26.893351
232.640055	8621.662565	26.898368
233.188423	8633.146258	26.903386
233.461080	8656.626659	26.908404
233.726297	8670.542136	26.913421
233.987500	8664.797186	26.918439
234.161610	8696.623310	26.923456
234.655468	8708.575292	26.928474
234.910576	8714.519699	26.933492
234.756952	8712.125323	26.938509
234.897080	8719.438357	26.943527
235.195989	8754.635010	26.948544
235.610125	8762.346615	26.953562
235.672445	8773.548687	26.958580
236.014376	8796.274655	26.963597
236.261032	8779.480897	26.968615
236.321378	8814.512310	26.973632
236.848762	8822.264123	26.978650
236.980736	8825.998940	26.983668
237.001253	8844.150084	26.988685
237.474416	8860.506973	26.993703
237.879675	8879.229881	26.998720
238.458881	8851.378312	27.003738
238.425086	8864.782943	27.008756
238.544077	8897.999676	27.013773
239.063292	8882.590962	27.018791
238.651948	8886.972283	27.023808
238.950090	8918.441530	27.028826
239.530101	8893.055889	27.033844
239.573309	8940.573251	27.038861
239.848819	8934.009118	27.043879
240.112574	8947.708297	27.048896
240.034746	8953.050782	27.053914
240.814829	8945.716884	27.058932
240.774038	8985.658542	27.063949
240.816737	8991.042418	27.068967
241.149103	8984.150111	27.073984
241.177608	9026.975838	27.079002
241.755016	9004.322157	27.084020
241.388021	9057.956949	27.089037
241.971440	9043.360150	27.094055
242.296789	9081.429097	27.099072
242.502148	9070.831789	27.104090
242.799010	9094.447517	27.109108
243.227145	9082.212546	27.114125
243.402182	9143.303725	27.119143
243.243282	9139.080165	27.124160
243.778363	9129.082600	27.129178
243.803271	9178.586642	27.134196
244.109636	9159.613823	27.139213
244.678344	9204.102061	27.144231
244.892859	9190.670720	27.149248
245.085047	9230.682518	27.154266
245.535164	9223.158327	27.159284
245.564358	9246.555710	27.164301
246.182081	9251.115003	27.169319
246.595594	9262.279162	27.174336
246.588006	9259.266903	27.179354
246.963746	9262.689125	27.184372
246.522609	9269.264895	27.189389
247.492805	9293.917776	27.194407
247.364031	9299.208699	27.199424
247.888915	9298.556501	27.204442
247.854236	9334.140170	27.209460
247.836395	9314.787999	27.214477
248.415644	9345.784465	27.219495
248.641797	9347.829443	27.224512
248.755325	9363.595009	27.229530
248.869185	9383.760607	27.234548
249.376302	9401.456348	27.239565
249.298964	9397.466019	27.244583
249.609024	9415.821547	27.249600
249.756493	9432.879804	27.254618
250.244567	9443.881518	27.259636
250.460989	9459.449396	27.264653
250.958510	9457.366597	27.269671
250.879099	9470.001560	27.274688
251.403324	9486.308898	27.279706
251.836469	9510.662551	27.284724
251.981474	9503.260437	27.289741
252.061910	9501.739489	27.294759
252.491103	9527.180939	27.299776
252.572928	9524.781556	27.304794
253.192634	9522.710747	27.309812
252.772563	9530.438482	27.314829
253.133402	9558.917411	27.319847
253.461149	9546.811386	27.324864
253.442111	9570.954711	27.329882
253.980389	9579.472839	27.334900
254.235781	9610.792579	27.339917
254.419913	9585.795850	27.344935
254.475687	9633.903607	27.349952
255.133468	9619.521431	27.354970
255.101841	9641.897457	27.359988
255.142932	9659.533228	27.365005
255.518283	9659.904656	27.370023
255.491413	9697.140900	27.375040
255.878737	9696.537372	27.380058
256.527223	9723.222186	27.385076
256.331103	9756.975417	27.390093
256.992916	9735.272367	27.395111
257.380080	9768.022548	27.400128
257.021243	9772.452411	27.405146
258.174181	9747.167592	27.410164
257.968593	9809.976313	27.415181
258.535485	9784.977259	27.420199
258.550891	9828.046201	27.425216
258.687768	9820.708969	27.430234
259.380043	9823.980923	27.435252
259.431247	9852.044291	27.440269
259.902967	9863.358980	27.445287
260.005009	9862.213468	27.450304
260.433508	9887.522648	27.455322
260.402859	9872.858072	27.460340
260.768682	9893.820324	27.465357
260.717808	9903.669636	27.470375
261.237412	9906.197137	27.475392
261.076561	9956.391641	27.480410
261.642935	9939.553493	27.485428
261.981019	9949.825988	27.490445
262.523619	9973.920174	27.495463
262.680529	9988.958635	27.500480
263.005303	9977.714452	27.505498
263.366359	9997.327593	27.510516
262.964719	9994.245398	27.515533
263.569449	10012.490552	27.520551
263.658185	10011.891721	27.525568
264.062384	10047.062043	27.530586
264.278308	10054.840152	27.535604
264.185812	10067.671688	27.540621
264.596054	10078.976274	27.545639
264.940372	10090.850905	27.550656
265.065240	10109.076267	27.555674
265.443135	10120.349447	27.560692
265.489420	10135.027161	27.565709
265.747144	10134.650461	27.570727
265.938153	10174.051531	27.575744
266.009314	10178.012797	27.580762
266.810145	10188.527658	27.585780
266.993259	10215.370952	27.590797
267.327008	10221.198762	27.595815
267.387098	10249.292540	27.600832
267.246479	10250.430896	27.605850
267.818582	10254.381583	27.610868
268.349913	10280.873981	27.615885
268.686213	10298.782562	27.620903
268.793240	10317.069649	27.625920
269.271497	10313.627564	27.630938
269.483542	10340.784406	27.635956
269.908358	10336.163296	27.640973
270.044506	10353.246441	27.645991
270.680343	10361.195834	27.651008
270.557316	10378.590253	27.656026
270.982054	10374.094272	27.661044
271.079621	10392.003637	27.666061
271.144094	10403.650438	27.671079
271.878043	10418.681556	27.676096
271.861514	10441.475824	27.681114
272.498297	10440.648749	27.686132
272.379564	10451.535453	27.691149
272.843886	10472.905422	27.696167
272.987203	10481.583432	27.701184
273.435052	10497.263060	27.706202
273.636308	10500.312026	27.711220
273.936781	10522.250412	27.716237
274.255481	10520.251855	27.721255
274.616824	10539.478859	27.726272
274.819163	10549.473959	27.731290
275.173675	10563.112542	27.736308
275.490820	10572.059590	27.741325
275.280319	10587.097011	27.746343
275.802689	10596.561069	27.751360
275.667857	10602.404303	27.756378
276.377081	10624.280438	27.761396
276.387679	10645.213797	27.766413
276.449725	10644.601489	27.771431
276.877490	10680.919723	27.776448
277.124343	10677.429449	27.781466
277.394024	10703.115928	27.786484
277.481119	10718.507015	27.791501
277.940878	10733.332287	27.796519
278.724541	10728.279645	27.801536
278.350147	10779.490342	27.806554
279.190059	10772.602893	27.811572
279.515558	10797.111950	27.816589
279.463882	10811.844895	27.821607
280.163941	10813.305353	27.826624
280.515128	10824.647070	27.831642
280.479081	10835.320580	27.836660
280.804788	10847.256230	27.841677
281.099832	10843.111325	27.846695
281.359119	10860.035333	27.851712
281.380178	10876.155637	27.856730
281.871654	10872.377636	27.861748
281.941808	10899.951999	27.866765
282.301937	10896.526648	27.871783
282.497314	10909.732092	27.876800
282.913021	10928.788809	27.881818
282.754164	10942.818072	27.886836
283.165963	10953.082263	27.891853
283.594211	10969.082672	27.896871
283.779773	10989.802494	27.901888
283.941667	11001.011214	27.906906
284.575717	11014.227102	27.911924
284.854122	11041.437200	27.916941
285.064498	11050.316556	27.921959
285.595593	11060.110455	27.926976
285.494144	11092.617164	27.931994
285.997501	11088.030137	27.937012
286.318002	11101.743496	27.942029
286.770023	11105.041449	27.947047
287.107137	11121.792010	27.952064
286.959867	11145.237004	27.957082
287.613334	11149.904136	27.962100
287.762008	11171.340171	27.967117
287.774250	11176.294860	27.972135
288.517828	11186.693244	27.977152
288.633451	11200.569601	27.982170
288.999708	11208.735565	27.987188
289.041267	11230.589546	27.992205
289.362268	11242.330687	27.997223
289.730883	11242.023256	28.002240
289.679740	11263.302584	28.007258
290.154856	11289.264650	28.012276
290.381527	11294.317813	28.017293
290.508014	11321.167778	28.022311
290.999153	11344.932775	28.027328
291.340969	11366.841014	28.032346
291.695202	11365.032262	28.037364
291.869602	11386.740552	28.042381
292.262699	11400.858162	28.047399
292.824036	11415.158320	28.052416
292.705629	11430.429420	28.057434
293.029341	11444.208690	28.062452
293.170668	11453.484935	28.067469
293.380293	11479.466429	28.072487
294.180603	11495.938162	28.077504
294.419331	11526.884418	28.082522
294.631120	11523.835952	28.087540
294.897234	11543.950274	28.092557
294.904527	11572.348499	28.097575
295.553976	11570.901140	28.102592
295.581571	11582.028991	28.107610
296.177865	11592.444839	28.112628
296.456917	11611.356958	28.117645
296.339426	11615.423442	28.122663
296.597487	11631.799949	28.127680
296.557951	11651.433455	28.132698
297.134408	11675.969268	28.137716
297.362559	11681.249780	28.142733
297.501509	11695.362135	28.147751
298.086373	11731.694462	28.152768
298.389018	11732.036618	28.157786
298.631733	11748.369656	28.162804
299.058280	11778.065784	28.167821
299.384594	11792.834277	28.172839
299.830538	11784.560617	28.177856
299.646006	11841.141031	28.182874
300.255995	11825.930121	28.187892
300.568886	11874.532557	28.192909
300.543491	11867.832131	28.197927
301.253542	11897.255848	28.202944
301.420120	11923.477542	28.207962
301.814010	11936.440135	28.212980
302.438857	11972.321197	28.217997
302.590016	11964.264823	28.223015
302.834157	12000.525783	28.228032
302.984953	11993.018819	28.233050
303.484606	12005.186214	28.238068
303.895353	12033.091264	28.243085
304.128293	12039.721537	28.248103
304.700315	12046.498468	28.253120
304.827181	12071.573705	28.258138
305.077114	12097.839478	28.263156
305.523093	12093.221948	28.268173
305.426361	12109.977629	28.273191
305.812795	12136.707527	28.278208
305.783108	12161.040084	28.283226
306.363881	12176.647351	28.288244
306.889362	12190.177719	28.293261
307.052122	12200.120408	28.298279
307.626672	12210.446492	28.303296
307.681015	12225.207992	28.308314
307.880950	12232.795571	28.313332
308.441644	12248.175700	28.318349
308.817700	12262.433983	28.323367
309.132530	12268.883856	28.328384
309.293751	12308.147282	28.333402
309.733569	12310.434293	28.338420
310.430634	12324.041721	28.343437
310.054509	12333.590272	28.348455
310.581214	12372.273387	28.353472
310.534823	12378.984537	28.358490
310.218952	12405.175935	28.363508
310.990971	12426.652531	28.368525
311.245420	12435.056778	28.373543
311.954487	12462.382220	28.378560
311.923146	12480.634165	28.383578
312.345211	12496.340850	28.388596
313.025426	12508.515688	28.393613
313.205307	12540.365557	28.398631
313.469610	12543.659123	28.403648
313.795822	12535.335667	28.408666
313.879315	12578.304006	28.413684
314.498402	12576.395054	28.418701
314.372720	12595.300502	28.423719
315.264407	12617.037911	28.428736
315.119595	12640.395884	28.433754
315.718728	12657.688446	28.438772
315.927867	12661.161629	28.443789
315.852860	12686.695876	28.448807
316.323519	12702.392473	28.453824
316.694619	12719.289729	28.458842
316.726348	12736.429012	28.463860
317.554571	12753.767030	28.468877
317.869763	12783.006688	28.473895
318.450900	12788.334835	28.478912
318.704334	12810.565438	28.483930
318.808501	12832.030009	28.488948
319.193211	12834.451428	28.493965
318.912016	12859.592416	28.498983
319.786226	12868.607502	28.504000
320.036464	12884.645209	28.509018
320.015870	12920.957847	28.514036
320.655045	12925.458203	28.519053
320.973973	12950.277203	28.524071
321.540158	12954.973778	28.529088
321.880359	12981.910300	28.534106
322.310034	12987.364393	28.539124
322.614586	13004.531533	28.544141
322.720395	13021.059553	28.549159
323.387178	13036.496781	28.554176
323.594531	13050.056391	28.559194
323.833199	13061.556263	28.564212
324.502581	13069.384682	28.569229
324.476635	13097.858359	28.574247
324.817812	13106.155884	28.579264
324.891055	13125.415579	28.584282
325.084135	13137.296065	28.589300
325.570005	13149.625779	28.594317
325.362961	13187.522736	28.599335
325.883862	13201.979020	28.604352
326.292131	13219.032073	28.609370
326.347700	13230.723206	28.614388
326.913557	13265.394144	28.619405
327.270637	13281.501432	28.624423
327.764239	13295.622513	28.629440
327.965428	13330.800184	28.634458
328.054556	13344.395822	28.639476
328.581175	13352.658811	28.644493
328.650988	13390.612704	28.649511
329.119205	13394.135089	28.654528
329.426765	13427.625545	28.659546
329.588962	13438.466074	28.664564
330.256053	13460.852887	28.669581
330.361676	13471.540307	28.674599
330.622950	13517.507530	28.679616
331.033329	13517.892782	28.684634
331.017074	13543.951601	28.689652
331.754542	13566.446605	28.694669
332.183362	13587.968733	28.699687
332.653833	13605.269703	28.704704
332.846806	13639.414110	28.709722
333.181961	13637.241137	28.714740
333.666865	13655.988601	28.719757
333.860544	13679.250728	28.724775
334.440142	13694.382551	28.729792
334.650732	13716.559519	28.734810
334.711829	13726.016721	28.739828
335.448524	13752.170195	28.744845
335.436974	13764.964899	28.749863
335.894102	13777.966325	28.754880
336.333270	13786.283438	28.759898
336.423283	13834.125763	28.764916
337.155153	13834.481632	28.769933
337.264014	13846.405711	28.774951
337.798225	13868.988071	28.779968
337.932827	13888.532364	28.784986
338.435516	13913.485117	28.790004
338.835217	13932.541784	28.795021
339.168740	13952.495560	28.800039
339.239613	13960.637877	28.805056
339.736831	13988.981921	28.810074
339.746242	13995.782005	28.815092
340.243467	14019.211564	28.820109
340.325535	14061.920350	28.825127
340.486299	14062.686637	28.830144
341.010708	14090.326453	28.835162
341.189825	14141.804843	28.840180
341.624919	14117.063414	28.845197
342.178160	14184.452383	28.850215
342.720069	14206.445607	28.855232
342.652188	14211.347639	28.860250
343.327995	14242.718907	28.865268
343.826188	14263.475446	28.870285
344.065127	14279.532269	28.875303
344.808856	14290.204665	28.880320
345.086328	14315.359475	28.885338
345.199564	14329.255410	28.890356
345.871070	14346.306056	28.895373
345.929673	14357.096545	28.900391
346.438726	14384.725469	28.905408
347.001749	14407.881927	28.910426
346.949395	14403.978193	28.915444
347.418430	14432.129382	28.920461
347.725405	14451.854249	28.925479
348.226484	14455.996184	28.930496
348.237476	14459.175664	28.935514
348.275305	14507.576592	28.940532
349.071684	14492.499241	28.945549
348.720224	14535.669944	28.950567
349.449048	14534.611745	28.955584
349.742739	14552.386829	28.960602
349.751684	14590.568310	28.965620
349.894070	14606.928289	28.970637
350.226600	14614.934890	28.975655
350.844109	14662.308640	28.980672
351.347355	14676.682753	28.985690
351.403345	14697.570774	28.990708
352.037932	14736.253936	28.995725
352.174949	14761.979855	29.000743
352.553456	14782.541073	29.005760
353.058444	14794.286849	29.010778
353.227950	14855.449402	29.015796
353.799870	14867.626190	29.020813
353.826852	14871.119664	29.025831
354.337927	14894.508880	29.030848
355.007015	14911.616341	29.035866
355.217132	14957.878072	29.040884
355.487661	14969.049488	29.045901
355.949310	14994.943498	29.050919
356.465470	15018.003162	29.055936
357.326130	15027.082724	29.060954
357.282510	15055.338509	29.065972
358.036626	15067.569080	29.070989
358.127907	15081.618277	29.076007
358.510387	15121.956388	29.081024
359.052871	15132.141397	29.086042
358.893110	15146.179196	29.091060
359.412704	15186.140195	29.096077
359.658307	15177.421559	29.101095
359.954337	15216.230051	29.106112
360.629782	15209.027184	29.111130
360.952935	15286.502459	29.116148
361.350104	15272.694299	29.121165
361.807610	15299.990062	29.126183
362.398232	15299.841149	29.131200
362.583879	15329.209861	29.136218
362.902763	15355.489262	29.141236
363.136494	15361.086741	29.146253
363.496015	15382.242906	29.151271
363.613209	15418.391225	29.156288
364.086136	15432.152708	29.161306
364.345682	15441.587416	29.166324
364.590479	15483.186741	29.171341
364.938706	15487.103964	29.176359
365.149668	15521.070809	29.181376
366.061660	15549.403515	29.186394
365.931628	15574.830217	29.191412
366.532894	15586.807571	29.196429
367.059696	15604.852969	29.201447
367.356282	15633.030705	29.206464
367.743253	15646.974354	29.211482
367.660404	15672.082834	29.216500
368.555391	15684.486594	29.221517
368.950823	15711.385681	29.226535
369.000903	15722.836729	29.231552
369.283621	15736.447042	29.236570
369.570887	15767.709975	29.241588
370.144477	15783.605424	29.246605
370.622019	15803.909467	29.251623
370.692701	15836.912050	29.256640
371.119005	15850.180449	29.261658
371.533420	15877.782185	29.266676
372.088812	15881.993111	29.271693
372.180871	15920.651771	29.276711
372.736230	15937.190132	29.281728
373.077093	15951.070651	29.286746
373.621601	15976.692045	29.291764
373.876136	15991.295878	29.296781
374.262919	16027.644065	29.301799
374.485675	16040.085963	29.306816
374.584833	16061.854538	29.311834
375.018806	16102.792826	29.316852
375.762307	16121.449665	29.321869
376.094662	16144.553113	29.326887
376.335670	16182.113478	29.331904
377.019192	16183.665525	29.336922
377.390586	16222.483546	29.341940
377.501586	16233.678455	29.346957
378.089227	16246.746911	29.351975
379.758047	16255.112108	29.356992
381.147238	16229.425510	29.362010
381.373675	16216.672981	29.367028
381.596473	16199.615242	29.372045
382.034459	16207.510914	29.377063
381.941882	16214.210242	29.382080
382.520432	16204.266309	29.387098
382.554636	16200.508336	29.392116
382.483000	16208.614727	29.397133
382.733402	16219.689594	29.402151
383.182495	16232.853137	29.407168
383.169206	16234.781347	29.412186
383.157368	16270.102467	29.417204
383.455584	16267.643337	29.422221
383.829357	16293.068194	29.427239
383.782995	16313.198665	29.432256
384.036557	16357.534368	29.437274
384.466574	16378.744546	29.442292
384.611853	16392.010569	29.447309
385.198726	16436.974584	29.452327
385.370516	16475.119447	29.457344
385.976491	16498.510684	29.462362
386.175907	16531.619718	29.467380
386.489951	16548.144546	29.472397
386.885966	16608.613118	29.477415
386.956492	16625.914924	29.482432
387.753770	16656.474756	29.487450
388.500619	16684.901036	29.492468
388.729508	16715.089022	29.497485
389.211882	16734.316404	29.502503
389.351493	16768.452276	29.507520
390.297062	16790.362857	29.512538
390.515234	16801.200592	29.517556
391.050083	16818.253251	29.522573
391.610175	16843.702471	29.527591
391.354197	16867.228869	29.532608
392.122503	16877.904200	29.537626
392.899330	16905.134323	29.542644
393.106808	16910.090271	29.547661
393.660808	16942.328031	29.552679
393.597392	16955.155604	29.557696
393.830709	16978.648685	29.562714
394.221175	17008.286162	29.567732
394.694144	17030.749313	29.572749
395.030069	17059.567914	29.577767
395.174894	17099.315889	29.582784
395.457414	17126.818262	29.587802
396.067435	17158.882210	29.592820
396.550289	17179.879976	29.597837
396.969697	17211.093194	29.602855
397.220993	17244.179153	29.607872
398.024792	17267.412296	29.612890
398.116647	17286.777000	29.617908
398.561320	17331.269480	29.622925
399.326886	17344.936454	29.627943
399.316790	17366.572818	29.632960
399.890178	17392.800092	29.637978
400.478910	17428.922574	29.642996
400.564383	17456.731124	29.648013
401.287220	17467.648939	29.653031
401.207153	17519.201399	29.658048
402.181945	17508.016425	29.663066
402.226873	17573.939190	29.668084
403.232460	17582.388586	29.673101
403.399027	17594.121260	29.678119
403.470924	17640.050703	29.683136
404.384046	17654.819758	29.688154
404.363978	17664.561692	29.693172
404.748671	17714.044814	29.698189
405.438803	17725.451459	29.703207
405.469936	17758.269486	29.708224
405.939806	17781.812113	29.713242
406.282382	17815.329605	29.718260
406.699691	17833.816804	29.723277
406.932963	17873.376305	29.728295
407.290872	17904.534586	29.733312
408.108937	17934.482655	29.738330
408.392012	17940.322319	29.743348
408.895278	17986.931261	29.748365
409.247092	18004.010268	29.753383
409.539106	18025.771059	29.758400
409.909424	18051.641671	29.763418
410.443483	18068.790525	29.768436
410.441188	18100.703813	29.773453
411.343524	18106.114169	29.778471
411.609406	18140.470144	29.783488
412.209484	18159.486858	29.788506
412.412704	18186.900804	29.793524
412.801928	18201.325732	29.798541
413.328384	18225.102530	29.803559
413.845114	18255.024830	29.808576
414.283752	18270.695456	29.813594
414.437389	18303.270516	29.818612
414.942125	18334.186587	29.823629
415.599250	18341.676604	29.828647
415.827161	18362.377635	29.833664
416.112146	18398.494880	29.838682
416.398508	18420.249252	29.843700
416.443187	18433.778921	29.848717
417.625465	18477.903235	29.853735
417.770514	18508.763977	29.858752
418.854411	18511.691252	29.863770
418.549891	18550.990146	29.868788
419.121026	18563.578571	29.873805
419.663430	18598.832437	29.878823
419.830604	18623.183234	29.883840
420.267845	18645.913877	29.888858
420.560064	18664.947197	29.893876
421.122988	18696.129128	29.898893
421.707884	18725.941871	29.903911
422.221125	18751.383398	29.908928
422.620677	18777.213950	29.913946
422.929505	18812.831112	29.918964
423.098870	18841.236261	29.923981
423.543529	18860.109704	29.928999
424.029640	18888.611715	29.934016
424.517770	18911.602359	29.939034
425.198364	18941.308535	29.944052
425.653747	18983.230786	29.949069
425.832618	18993.554464	29.954087
426.383861	19028.966958	29.959104
426.626254	19058.448685	29.964122
427.127687	19080.942174	29.969140
427.464747	19115.543302	29.974157
428.142069	19133.043357	29.979175
428.215514	19160.695847	29.984192
428.822042	19189.705224	29.989210
429.259723	19209.360937	29.994228
429.092235	19249.712232	29.999245
430.278745	19276.558028	30.004263
430.455905	19306.672296	30.009280
430.749344	19332.489575	30.014298
431.380777	19358.158550	30.019316
431.731155	19399.609265	30.024333
432.146349	19415.291873	30.029351
432.769227	19447.794956	30.034368
433.062205	19473.091651	30.039386
433.339554	19495.057637	30.044404
433.960449	19513.386840	30.049421
434.504018	19539.608726	30.054439
434.524984	19574.344314	30.059456
435.027994	19593.268410	30.064474
435.801005	19600.902008	30.069492
435.817157	19644.159483	30.074509
436.376204	19670.271637	30.079527
436.619171	19689.093574	30.084544
437.087270	19733.914823	30.089562
437.443261	19755.837542	30.094580
437.947077	19785.835724	30.099597
438.263395	19811.393047	30.104615
438.664326	19860.998144	30.109632
439.303643	19864.959989	30.114650
439.896173	19943.499994	30.119668
439.666923	19961.998254	30.124685
440.841874	19953.711601	30.129703
441.045186	20024.036199	30.134720
441.474572	20052.643090	30.139738
442.018493	20072.243988	30.144756
442.254518	20108.967541	30.149773
443.133731	20135.021982	30.154791
443.737452	20169.621549	30.159808
444.045511	20195.438322	30.164826
444.736669	20211.755783	30.169844
444.726267	20246.137590	30.174861
445.354675	20276.498004	30.179879
446.019995	20281.631526	30.184896
446.241367	20323.379685	30.189914
447.022622	20343.184081	30.194932
447.188806	20369.094619	30.199949
447.946970	20391.969618	30.204967
448.167329	20431.573902	30.209984
448.144611	20455.146701	30.215002
448.685400	20480.765430	30.220020
448.929614	20517.381932	30.225037
449.358553	20550.390712	30.230055
450.143775	20588.772585	30.235072
450.352447	20622.761214	30.240090
450.871778	20653.890622	30.245108
451.337742	20693.436355	30.250125
451.772917	20713.327074	30.255143
452.308930	20759.713089	30.260160
452.502060	20786.557155	30.265178
453.401557	20813.913613	30.270196
453.586250	20854.772061	30.275213
454.143223	20893.972258	30.280231
454.728467	20918.583301	30.285248
454.899633	20948.013793	30.290266
455.352247	20983.251136	30.295284
455.797112	21017.951919	30.300301
456.415541	21045.098408	30.305319
456.958327	21077.570005	30.310336
457.094720	21100.747894	30.315354
458.157332	21114.329548	30.320372
458.477818	21148.387736	30.325389
458.939667	21168.424414	30.330407
459.407969	21198.334102	30.335424
459.854358	21227.065258	30.340442
460.524531	21238.469814	30.345460
460.658258	21265.693910	30.350477
461.097315	21285.892664	30.355495
461.596439	21309.639159	30.360512
461.660150	21343.481945	30.365530
462.555347	21363.944404	30.370548
462.401310	21398.596148	30.375565
463.000672	21436.260765	30.380583
463.170092	21480.635305	30.385600
463.665045	21488.610656	30.390618
464.450335	21560.184302	30.395636
464.819948	21572.640322	30.400653
465.197527	21611.096737	30.405671
465.790139	21662.693911	30.410688
466.252256	21692.191275	30.415706
467.003561	21713.352049	30.420724
467.087921	21756.439093	30.425741
467.850780	21795.718214	30.430759
468.432203	21809.023529	30.435776
468.589299	21851.206941	30.440794
469.095239	21878.182207	30.445812
469.451230	21932.175133	30.450829
469.995255	21935.838860	30.455847
470.553517	21995.304063	30.460864
471.084181	22027.816181	30.465882
471.929099	22054.558179	30.470900
471.964371	22102.025002	30.475917
472.671313	22099.574093	30.480935
473.408380	22174.297480	30.485952
473.876185	22160.832614	30.490970
474.567850	22223.300926	30.495988
474.727607	22233.217887	30.501005
474.845818	22288.890445	30.506023
476.120965	22304.909141	30.511040
476.398279	22324.623073	30.516058
476.670707	22371.389778	30.521076
476.941503	22382.557943	30.526093
477.054330	22429.197454	30.531111
478.179178	22450.675395	30.536128
478.399578	22478.024819	30.541146
478.759442	22504.085622	30.546164
478.990457	22552.199155	30.551181
479.805623	22568.834058	30.556199
480.121087	22619.186077	30.561216
480.598516	22667.325286	30.566234
480.678805	22674.839615	30.571252
481.357821	22708.632197	30.576269
482.101528	22752.497456	30.581287
482.900326	22800.103071	30.586304
483.215834	22817.239997	30.591322
483.949371	22826.173562	30.596340
484.120601	22853.117186	30.601357
484.401182	22883.875164	30.606375
484.840584	22924.558601	30.611392
485.066942	22956.409902	30.616410
486.098461	22969.555498	30.621428
486.225043	23017.479154	30.626445
486.525505	23048.827361	30.631463
487.149715	23064.990712	30.636480
487.362565	23117.316326	30.641498
487.996267	23152.267795	30.646516
488.308022	23193.535412	30.651533
489.180450	23231.588505	30.656551
489.501149	23260.538730	30.661568
489.705182	23300.435982	30.666586
490.367700	23335.962964	30.671604
490.986874	23373.296678	30.676621
491.617485	23410.502637	30.681639
492.039515	23449.295924	30.686656
492.633145	23479.897282	30.691674
493.257874	23522.344616	30.696692
493.857331	23558.865911	30.701709
494.235583	23576.788401	30.706727
494.590741	23605.139094	30.711744
495.224594	23652.200935	30.716762
496.007770	23674.471440	30.721780
496.393952	23714.782589	30.726797
496.676177	23738.181355	30.731815
496.978667	23778.780891	30.736832
497.934125	23818.875591	30.741850
498.483148	23838.489841	30.746868
499.069715	23876.154452	30.751885
499.591660	23909.779289	30.756903
500.128389	23938.205625	30.761920
500.628955	23964.919875	30.766938
501.163670	23995.176380	30.771956
501.631004	24026.798465	30.776973
501.942159	24064.116715	30.781991
502.216682	24080.777124	30.787008
502.528637	24121.798221	30.792026
502.718681	24147.303546	30.797044
503.386614	24202.985049	30.802061
503.865160	24243.429336	30.807079
504.829963	24280.501395	30.812096
505.051354	24323.624006	30.817114
505.760074	24361.752373	30.822132
506.304467	24390.891154	30.827149
507.011884	24437.146468	30.832167
507.533792	24462.278842	30.837184
507.708261	24499.110252	30.842202
508.342193	24521.586109	30.847220
508.825492	24565.914571	30.852237
509.068333	24610.947065	30.857255
510.005263	24626.428894	30.862272
510.242580	24672.462819	30.867290
510.664557	24696.693813	30.872308
510.931488	24723.659240	30.877325
511.106787	24748.184036	30.882343
511.855121	24790.225948	30.887360
512.173531	24827.648810	30.892378
512.930394	24865.377651	30.897396
513.640436	24905.257403	30.902413
514.084916	24949.466296	30.907431
514.655528	24979.476342	30.912448
514.591300	25021.709748	30.917466
515.664665	25059.045974	30.922484
516.231880	25099.128564	30.927501
516.673967	25137.148449	30.932519
517.048556	25174.242572	30.937536
517.416512	25216.473027	30.942554
517.968645	25243.792491	30.947572
518.327097	25286.913203	30.952589
518.525043	25344.713002	30.957607
519.465360	25383.428448	30.962624
519.889423	25425.433103	30.967642
520.579157	25470.342480	30.972660
521.366554	25515.946181	30.977677
521.826577	25547.704795	30.982695
522.549257	25586.943806	30.987712
522.880838	25624.112784	30.992730
523.298162	25662.831082	30.997748
524.076313	25690.524938	31.002765
524.542887	25750.461541	31.007783
525.394209	25764.363713	31.012800
525.968525	25817.101455	31.017818
526.155690	25848.253445	31.022836
526.771722	25888.164812	31.027853
527.162528	25920.393670	31.032871
528.019208	25953.236098	31.037888
528.512998	26003.906014	31.042906
529.182098	26034.691700	31.047924
529.920506	26055.079683	31.052941
529.944749	26098.414951	31.057959
530.460687	26138.884874	31.062976
531.206053	26174.544444	31.067994
531.729105	26198.099103	31.073012
532.586930	26236.626518	31.078029
532.936069	26264.435401	31.083047
533.458820	26301.974117	31.088064
533.868984	26347.910494	31.093082
534.342040	26377.195832	31.098100
534.879892	26409.065079	31.103117
535.104630	26447.206208	31.108135
535.936559	26473.396850	31.113152
536.354924	26513.063962	31.118170
536.727180	26568.531397	31.123188
537.273934	26594.300502	31.128205
537.618085	26643.204831	31.133223
538.415042	26667.115964	31.138240
538.818557	26715.779446	31.143258
539.399688	26748.457848	31.148276
539.977981	26771.923410	31.153293
540.208950	26821.526972	31.158311
540.929217	26848.611269	31.163328
541.430493	26888.019518	31.168346
541.926758	26926.421839	31.173364
542.729096	26968.025225	31.178381
543.047000	27001.425954	31.183399
543.536625	27037.609539	31.188416
543.884449	27080.977057	31.193434
544.403226	27124.608168	31.198452
544.990156	27153.455302	31.203469
545.302607	27209.873559	31.208487
546.020742	27250.062763	31.213504
546.527090	27300.250258	31.218522
546.728162	27344.790517	31.223540
547.456712	27382.729925	31.228557
547.859185	27430.562996	31.233575
548.940567	27479.534427	31.238592
549.328486	27529.764349	31.243610
549.836184	27563.181707	31.248628
550.790419	27606.975602	31.253645
551.159983	27655.530732	31.258663
551.986982	27694.271403	31.263680
552.678747	27741.293528	31.268698
553.165434	27778.301763	31.273716
554.122717	27817.516750	31.278733
554.274047	27845.275577	31.283751
554.469025	27881.865679	31.288768
555.238030	27934.772390	31.293786
555.778197	27981.707488	31.298804
556.352359	28023.837639	31.303821
556.823116	28069.027110	31.308839
557.521460	28096.292700	31.313856
558.196831	28143.624303	31.318874
558.736935	28177.155166	31.323892
559.857658	28212.134697	31.328909
559.954023	28246.989103	31.333927
560.714461	28278.516971	31.338944
561.195388	28318.157294	31.343962
561.427298	28366.401640	31.348980
562.350004	28391.736353	31.353997
562.378868	28435.464016	31.359015
563.249899	28477.655219	31.364032
563.718331	28520.265207	31.369050
563.923884	28575.268153	31.374068
564.573242	28601.845906	31.379085
565.250416	28646.503015	31.384103
566.035260	28686.576450	31.389120
566.568955	28742.161165	31.394138
566.899844	28778.106054	31.399156
567.497188	28818.376716	31.404173
568.099339	28861.199523	31.409191
568.567568	28899.229664	31.414208
569.240033	28931.390539	31.419226
569.804905	28968.028185	31.424244
570.024276	29018.091812	31.429261
570.581914	29049.716521	31.434279
571.296786	29084.012496	31.439296
571.439227	29135.106724	31.444314
571.820627	29187.951633	31.449332
572.764591	29225.441893	31.454349
573.264436	29274.593349	31.459367
573.557640	29320.958662	31.464384
574.382244	29377.074406	31.469402
574.982885	29414.862470	31.474420
575.549522	29450.095255	31.479437
576.468705	29515.342747	31.484455
577.098613	29549.364855	31.489472
577.451963	29593.113290	31.494490
578.155807	29645.407200	31.499508
579.094219	29685.236448	31.504525
579.297568	29732.562781	31.509543
579.797817	29774.996075	31.514560
580.705003	29824.052797	31.519578
581.142225	29867.344207	31.524596
581.890142	29911.894253	31.529613
582.245258	29951.760327	31.534631
583.005121	29991.743264	31.539648
583.537090	30032.848407	31.544666
583.972137	30083.139413	31.549684
584.882270	30119.173094	31.554701
585.493860	30167.493120	31.559719
585.949155	30212.928995	31.564736
586.785818	30250.900470	31.569754
587.175246	30292.886286	31.574772
587.714951	30337.049881	31.579789
588.269820	30381.597290	31.584807
588.992361	30427.785484	31.589824
589.809583	30462.053888	31.594842
589.923402	30522.133721	31.599860
590.453743	30563.294046	31.604877
591.082516	30612.666981	31.609895
591.487718	30650.443342	31.614912
592.044069	30707.522048	31.619930
592.873803	30740.074370	31.624948
593.569477	30807.342086	31.629965
594.160777	30837.299086	31.634983
594.625878	30894.971372	31.640000
595.079949	30957.067908	31.645018
595.644798	31000.067772	31.650036
596.200413	31038.623268	31.655053
596.838526	31093.557945	31.660071
597.502464	31149.937067	31.665088
598.258919	31192.766655	31.670106
598.876766	31250.149517	31.675124
599.614695	31286.640317	31.680141
599.785178	31326.039546	31.685159
600.364815	31384.778062	31.690176
601.334066	31413.788608	31.695194
601.621118	31459.749628	31.700212
602.162188	31493.337619	31.705229
602.910958	31552.771638	31.710247
603.327483	31598.041020	31.715264
604.078824	31640.067221	31.720282
604.568337	31690.318249	31.725300
605.115879	31730.102852	31.730317
605.592175	31774.568855	31.735335
606.138415	31824.938924	31.740352
606.994691	31876.430814	31.745370
607.420952	31919.264457	31.750388
608.093603	31963.759593	31.755405
608.561509	32022.184051	31.760423
609.032572	32068.453183	31.765440
609.886224	32122.721809	31.770458
610.253990	32184.121177	31.775476
611.410942	32232.530673	31.780493
611.667011	32281.213030	31.785511
612.727474	32324.613436	31.790528
613.319276	32373.620873	31.795546
613.970937	32430.296364	31.800564
614.687835	32463.133309	31.805581
615.211677	32500.781560	31.810599
615.692498	32556.893635	31.815616
616.597266	32606.326349	31.820634
617.141165	32650.482909	31.825652
618.061857	32685.641073	31.830669
618.529560	32739.516112	31.835687
619.200621	32786.513557	31.840704
620.107472	32827.909629	31.845722
620.304442	32871.489979	31.850740
620.994320	32907.205521	31.855757
621.907540	32963.563784	31.860775
622.081960	33003.198106	31.865792
622.722398	33037.604095	31.870810
623.254735	33096.860652	31.875828
623.807042	33146.767244	31.880845
624.378423	33188.681058	31.885863
625.176343	33240.252719	31.890880
625.579449	33288.757012	31.895898
625.757936	33355.436598	31.900916
626.429667	33396.561025	31.905933
627.337704	33449.767709	31.910951
627.902873	33515.874080	31.915968
628.857045	33561.908117	31.920986
629.297540	33623.871869	31.926004
629.963940	33658.345951	31.931021
630.325372	33726.980848	31.936039
630.969093	33773.692273	31.941056
631.814174	33831.342717	31.946074
632.592214	33893.434997	31.951092
633.301413	33940.560490	31.956109
633.781895	33987.460873	31.961127
634.365896	34034.918680	31.966144
635.164034	34075.192377	31.971162
635.667122	34133.350737	31.976180
636.423015	34155.254680	31.981197
637.349212	34197.045192	31.986215
637.525171	34245.451322	31.991232
638.214952	34296.217505	31.996250
638.381578	34341.551556	32.001268
639.250629	34378.947347	32.006285
639.920606	34433.910168	32.011303
640.319265	34484.308709	32.016320
641.027466	34526.866195	32.021338
641.601017	34608.655582	32.026356
642.369343	34647.439454	32.031373
642.983066	34713.873910	32.036391
643.567947	34761.294246	32.041408
644.384938	34807.526999	32.046426
644.778512	34880.411467	32.051444
645.863516	34910.423382	32.056461
646.371238	34966.550381	32.061479
646.872971	35021.915546	32.066496
647.909099	35075.586287	32.071514
647.979869	35130.899059	32.076532
648.752187	35185.830730	32.081549
649.809788	35242.656151	32.086567
650.321932	35303.177067	32.091584
651.050734	35340.434990	32.096602
651.667821	35421.518352	32.101620
652.073524	35461.306157	32.106637
652.828684	35507.837618	32.111655
654.027924	35560.421426	32.116672
654.339669	35613.444677	32.121690
654.738684	35679.366993	32.126708
655.621822	35732.490385	32.131725
656.291799	35785.130807	32.136743
656.888813	35843.784663	32.141760
657.792250	35887.083864	32.146778
658.456857	35944.188663	32.151796
659.022810	36000.722912	32.156813
659.861025	36046.932084	32.161831
660.184125	36102.452249	32.166848
661.146961	36144.347457	32.171866
661.723083	36212.551679	32.176884
662.346522	36254.578458	32.181901
663.141939	36306.628275	32.186919
663.598003	36367.338549	32.191936
664.563001	36412.147507	32.196954
665.115409	36475.718425	32.201972
665.371578	36521.972723	32.206989
666.561604	36577.630736	32.212007
666.897839	36631.728520	32.217024
667.982102	36679.144162	32.222042
668.271975	36733.383664	32.227060
668.758978	36792.756782	32.232077
669.813397	36828.834209	32.237095
670.116101	36880.858640	32.242112
670.945431	36923.425035	32.247130
671.442173	36979.128564	32.252148
671.949527	37028.598332	32.257165
672.892296	37064.134357	32.262183
673.414753	37121.481803	32.267200
674.039053	37167.212588	32.272218
674.407378	37244.067074	32.277236
675.187600	37286.047829	32.282253
675.807982	37337.729840	32.287271
676.137536	37400.761131	32.292288
676.797767	37463.418371	32.297306
677.538677	37518.241311	32.302324
678.071204	37582.505424	32.307341
678.863778	37647.630216	32.312359
679.583927	37714.245693	32.317376
680.544767	37775.385212	32.322394
680.957700	37836.350471	32.327412
681.848373	37891.876049	32.332429
682.791525	37951.547992	32.337447
683.212469	38021.301033	32.342464
684.032157	38073.688305	32.347482
684.508600	38135.628385	32.352500
685.172414	38202.770343	32.357517
686.009188	38263.735881	32.362535
686.735581	38330.797432	32.367552
687.699156	38382.957783	32.372570
688.107030	38451.626749	32.377588
689.057673	38504.943697	32.382605
689.717666	38558.228256	32.387623
690.473811	38628.225280	32.392640
690.932903	38677.127337	32.397658
691.907946	38739.026506	32.402676
692.483816	38801.689539	32.407693
693.020129	38867.700258	32.412711
693.812355	38924.889476	32.417728
694.427765	38980.560229	32.422746
695.548310	39048.416481	32.427764
696.180113	39103.867434	32.432781
697.171664	39148.200127	32.437799
697.494937	39207.309809	32.442816
698.329697	39259.152792	32.447834
699.369897	39315.922265	32.452852
699.926190	39372.622334	32.457869
700.503346	39428.475677	32.462887
701.062259	39486.135987	32.467904
702.102842	39532.518054	32.472922
702.780282	39589.004032	32.477940
703.230247	39648.115576	32.482957
704.496901	39697.727722	32.487975
704.819175	39753.460302	32.492992
705.488994	39801.830619	32.498010
706.086689	39863.514882	32.503028
706.523208	39923.332801	32.508045
707.308920	39980.681154	32.513063
707.735806	40026.801184	32.518080
708.717258	40080.422531	32.523098
709.281019	40144.330300	32.528116
709.734484	40194.486517	32.533133
710.491613	40247.186938	32.538151
711.171602	40315.878471	32.543168
711.432106	40376.639030	32.548186
712.517135	40433.329417	32.553204
712.781186	40493.643564	32.558221
713.490574	40558.415924	32.563239
714.189122	40635.927069	32.568256
715.130813	40690.808750	32.573274
715.749018	40751.023266	32.578292
716.336482	40830.748076	32.583309
717.487023	40902.680211	32.588327
717.940556	40971.236975	32.593344
718.653336	41028.455391	32.598362
719.466085	41104.023434	32.603380
720.459741	41162.676775	32.608397
721.125625	41224.523845	32.613415
721.551931	41293.748569	32.618432
722.558509	41363.612910	32.623450
723.402946	41425.662521	32.628468
724.095380	41495.299864	32.633485
724.712770	41556.818378	32.638503
725.267962	41614.136387	32.643520
726.504083	41673.434150	32.648538
727.130145	41742.751893	32.653556
727.552982	41800.037978	32.658573
728.725980	41881.175795	32.663591
729.263004	41951.281306	32.668608
730.249710	42002.125955	32.673626
731.152065	42070.032155	32.678644
731.279168	42139.777894	32.683661
732.578093	42202.461333	32.688679
733.228224	42269.818655	32.693696
734.048939	42323.620891	32.698714
734.952605	42382.198119	32.703732
735.447224	42455.062875	32.708749
736.154675	42500.821609	32.713767
736.770174	42571.453371	32.718784
737.545808	42630.830919	32.723802
738.392037	42700.171098	32.728820
738.904071	42774.977441	32.733837
739.757533	42832.141633	32.738855
740.509878	42893.605602	32.743872
741.073820	42956.238479	32.748890
741.864052	43018.154231	32.753908
742.484318	43086.532033	32.758925
743.167683	43146.692546	32.763943
743.885422	43229.852270	32.768960
744.869764	43299.226498	32.773978
745.778152	43352.002298	32.778996
746.036783	43434.185701	32.784013
746.843970	43495.078454	32.789031
747.620897	43552.594740	32.794048
748.148958	43614.257860	32.799066
749.104107	43682.376519	32.804084
749.974271	43737.727273	32.809101
750.718625	43780.625634	32.814119
751.191782	43878.725776	32.819136
752.075906	43926.488480	32.824154
752.951486	43988.435136	32.829172
753.617017	44065.859765	32.834189
754.324349	44129.190135	32.839207
754.970991	44187.243458	32.844224
755.686305	44242.185160	32.849242
756.513134	44317.724077	32.854260
757.279292	44387.957589	32.859277
758.031147	44430.635551	32.864295
758.805640	44507.950174	32.869312
759.517560	44579.145772	32.874330
760.572312	44639.271283	32.879348
761.374300	44718.033573	32.884365
762.004184	44780.608932	32.889383
762.846474	44836.481841	32.894400
763.224875	44914.514336	32.899418
764.110065	44975.563923	32.904436
764.971859	45043.759586	32.909453
765.844037	45111.001153	32.914471
766.512263	45186.916116	32.919488
767.046916	45253.489545	32.924506
767.873272	45332.326452	32.929524
768.734780	45408.381965	32.934541
769.444692	45454.397355	32.939559
770.608060	45558.122937	32.944576
771.237531	45598.009220	32.949594
771.988760	45679.926081	32.954612
772.854196	45761.153178	32.959629
773.665623	45810.967485	32.964647
774.429757	45897.975153	32.969664
775.234434	45951.876414	32.974682
776.193462	46035.367669	32.979700
776.537502	46099.053294	32.984717
777.710960	46160.512292	32.989735
778.125579	46232.989220	32.994752
779.098100	46294.840333	32.999770
780.122055	46369.874084	33.004788
780.878797	46428.750253	33.009805
782.114863	46497.592415	33.014823
782.475405	46568.312587	33.019840
783.401175	46637.031172	33.024858
784.398070	46686.638624	33.029876
785.053077	46775.352774	33.034893
785.689456	46825.813061	33.039911
786.251111	46876.231754	33.044928
786.568444	46969.348208	33.049946
787.761354	47023.638985	33.054964
788.355143	47088.175008	33.059981
789.646000	47160.298592	33.064999
790.269624	47230.121383	33.070016
790.394072	47297.856387	33.075034
791.451571	47341.909454	33.080052
791.731198	47447.856647	33.085069
792.613314	47483.097434	33.090087
793.155144	47585.763438	33.095104
793.891167	47636.756030	33.100122
794.965559	47702.047601	33.105140
795.418028	47792.376694	33.110157
796.471599	47844.909537	33.115175
797.325276	47939.296156	33.120192
797.810293	48030.807635	33.125210
799.079958	48098.252986	33.130228
799.932911	48176.527373	33.135245
800.949848	48239.066114	33.140263
801.114820	48321.763856	33.145280
802.419263	48369.812597	33.150298
803.085091	48482.917439	33.155316
803.553702	48543.913267	33.160333
804.055490	48634.680559	33.165351
805.341539	48693.407492	33.170368
805.816549	48821.065612	33.175386
807.018250	48854.933041	33.180404
807.836507	48972.317476	33.185421
808.519484	49017.620774	33.190439
809.377004	49117.399290	33.195456
810.697670	49190.255343	33.200474
811.745401	49265.379706	33.205492
812.177091	49341.732089	33.210509
813.516339	49392.636895	33.215527
814.329543	49495.580030	33.220544
815.134997	49552.398384	33.225562
816.120326	49613.760570	33.230580
816.834017	49709.882878	33.235597
817.586863	49745.454855	33.240615
818.278672	49843.957460	33.245632
819.281292	49893.939083	33.250650
819.795631	49952.247130	33.255668
820.472538	50041.330781	33.260685
821.668778	50125.554690	33.265703
822.701778	50197.280493	33.270720
823.277441	50272.301237	33.275738
824.477688	50325.865772	33.280756
825.370881	50397.630415	33.285773
825.739091	50485.266506	33.290791
826.651141	50553.106329	33.295808
827.195200	50623.084558	33.300826
828.070061	50675.856224	33.305844
828.781903	50789.668991	33.310861
829.704566	50843.926184	33.315879
830.727736	50913.406430	33.320896
830.968636	50998.139965	33.325914
831.901433	51070.320723	33.330932
832.565096	51172.186533	33.335949
833.470225	51213.641618	33.340967
834.449851	51317.124203	33.345984
835.086712	51378.333347	33.351002
835.551067	51429.960762	33.356020
836.308707	51524.949771	33.361037
837.285629	51595.613993	33.366055
838.518121	51664.574692	33.371072
839.196213	51743.403872	33.376090
840.433933	51811.862527	33.381108
840.988092	51880.184084	33.386125
842.012194	51976.723637	33.391143
842.895813	52027.471823	33.396160
843.415601	52125.717734	33.401178
844.290331	52173.936705	33.406196
844.642176	52279.074321	33.411213
845.656978	52320.776463	33.416231
846.830780	52438.139737	33.421248
847.380369	52503.576678	33.426266
848.589533	52580.936378	33.431284
849.350441	52672.333103	33.436301
850.567516	52743.894651	33.441319
851.070560	52840.464968	33.446336
851.610615	52901.899858	33.451354
853.270019	52974.635410	33.456372
853.746480	53078.239788	33.461389
854.715513	53126.578863	33.466407
855.636753	53243.646727	33.471424
856.522965	53301.701345	33.476442
857.052513	53403.730549	33.481460
857.943909	53456.409934	33.486477
858.866893	53573.337630	33.491495
859.802085	53616.346324	33.496512
860.493462	53731.897939	33.501530
861.524954	53776.842219	33.506548
862.539099	53896.124647	33.511565
863.248902	53955.449840	33.516583
864.300212	54040.621051	33.521600
864.844211	54134.360603	33.526618
866.041611	54184.225364	33.531636
866.799691	54308.411925	33.536653
867.659756	54354.464379	33.541671
868.425612	54454.564952	33.546688
869.194874	54561.833584	33.551706
870.509419	54616.601631	33.556724
871.513223	54719.639078	33.561741
872.559097	54793.442299	33.566759
873.588093	54850.942580	33.571776
873.770580	54947.947602	33.576794
875.255161	55007.579047	33.581812
876.092576	55091.734991	33.586829
876.948773	55168.385460	33.591847
877.821152	55242.704210	33.596864
878.393418	55326.979193	33.601882
879.329615	55408.112759	33.606900
880.349339	55483.444369	33.611917
880.800945	55560.817431	33.616935
881.822361	55627.443703	33.621952
882.688750	55692.409301	33.626970
883.552592	55780.958121	33.631988
884.409628	55844.098104	33.637005
884.991509	55903.996101	33.642023
885.720858	56000.439885	33.647040
886.241922	56082.264362	33.652058
887.365004	56152.632732	33.657076
888.145698	56244.000104	33.662093
889.061388	56299.641640	33.667111
890.202900	56413.591884	33.672128
890.969508	56494.293234	33.677146
891.980546	56571.843546	33.682164
892.727232	56642.084299	33.687181
893.264542	56752.325822	33.692199
894.929075	56818.134359	33.697216
895.397414	56917.064657	33.702234
896.768387	56963.152891	33.707252
897.600632	57080.013356	33.712269
898.090714	57155.874935	33.717287
899.277091	57264.822974	33.722304
900.213160	57320.518034	33.727322
901.070134	57429.522626	33.732340
902.182653	57514.870787	33.737357
902.766145	57588.477920	33.742375
904.238802	57674.094666	33.747392
904.988995	57758.854457	33.752410
905.847828	57828.125359	33.757428
906.759488	57929.506600	33.762445
907.432435	58010.560988	33.767463
908.365745	58082.854810	33.772480
909.304703	58188.501322	33.777498
910.540190	58258.945121	33.782516
911.336282	58365.417252	33.787533
912.121874	58443.440684	33.792551
913.134573	58502.719803	33.797568
914.036802	58593.826941	33.802586
914.946042	58698.969660	33.807604
916.049484	58783.472731	33.812621
916.645337	58868.034861	33.817639
917.730689	58960.251211	33.822656
918.399831	59028.679127	33.827674
919.616499	59148.727546	33.832692
920.414711	59200.317541	33.837709
921.572005	59319.154699	33.842727
922.684125	59384.438366	33.847744
923.846905	59448.160870	33.852762
924.705793	59560.688501	33.857780
925.979187	59620.766376	33.862797
926.415316	59699.674736	33.867815
927.571687	59786.718678	33.872832
928.588169	59862.643351	33.877850
929.296478	59935.911599	33.882868
930.164950	60040.140164	33.887885
930.634652	60105.181290	33.892903
932.127655	60166.637295	33.897920
932.458748	60281.469692	33.902938
933.220516	60319.378459	33.907956
934.751376	60397.477795	33.912973
934.926483	60463.934176	33.917991
936.147386	60561.794875	33.923008
937.021796	60623.821272	33.928026
937.531363	60706.157430	33.933044
938.554122	60823.235351	33.938061
939.263985	60880.063266	33.943079
940.450393	60975.402527	33.948096
941.226232	61064.792656	33.953114
942.163450	61136.488354	33.958132
942.960374	61263.595184	33.963149
943.474112	61348.279512	33.968167
945.261471	61413.908057	33.973184
946.020479	61552.269933	33.978202
946.713723	61631.878082	33.983220
947.984455	61718.521295	33.988237
948.652961	61836.246060	33.993255
949.894231	61910.236105	33.998272
950.631853	62012.630334	34.003290
951.188564	62119.165139	34.008308
952.736848	62185.996440	34.013325
953.530296	62335.122992	34.018343
954.488922	62396.099824	34.023360
955.698977	62523.638873	34.028378
956.323499	62595.273060	34.033396
957.460933	62703.427084	34.038413
958.424809	62813.822924	34.043431
959.844216	62891.748299	34.048448
960.450190	63023.570873	34.053466
961.797254	63075.529478	34.058484
962.984120	63152.630856	34.063501
963.406415	63290.932750	34.068519
964.524822	63355.278765	34.073536
965.514878	63461.846926	34.078554
966.641906	63566.789694	34.083572
967.771047	63627.860218	34.088589
968.576381	63759.754088	34.093607
970.092753	63816.699389	34.098624
970.856176	63927.045193	34.103642
971.707971	64012.000317	34.108660
972.884761	64114.996066	34.113677
973.495842	64197.883960	34.118695
974.513297	64297.574386	34.123712
975.095283	64364.759790	34.128730
976.458363	64464.203460	34.133748
977.353738	64591.076994	34.138765
978.110075	64661.062150	34.143783
979.430993	64743.059440	34.148800
980.339183	64880.142888	34.153818
981.218465	64955.614113	34.158836
982.316193	65044.753941	34.163853
983.619536	65128.170522	34.168871
984.511590	65229.948037	34.173888
985.628637	65286.778114	34.178906
985.992329	65380.220852	34.183924
987.005133	65462.456591	34.188941
987.835687	65545.242783	34.193959
989.153889	65627.196935	34.198976
989.963786	65727.123664	34.203994
990.879516	65812.215599	34.209012
992.045764	65878.438541	34.214029
992.329064	65996.300908	34.219047
993.584868	66066.818137	34.224064
994.329478	66186.787496	34.229082
995.499519	66246.697660	34.234100
996.732099	66343.203064	34.239117
997.442348	66498.616323	34.244135
998.351595	66572.652106	34.249152
999.190378	66657.270483	34.254170
1000.164310	66744.309169	34.259188
1001.577766	66878.224975	34.264205
1002.575995	66963.008834	34.269223
1003.469075	67073.314252	34.274240
1004.464293	67186.734093	34.279258
1005.566731	67277.071133	34.284276
1006.804002	67366.006882	34.289293
1007.457845	67494.751021	34.294311
1008.517842	67579.136106	34.299328
1009.602930	67710.617850	34.304346
1010.799496	67795.923403	34.309364
1012.116400	67898.102286	34.314381
1012.583031	68015.161328	34.319399
1013.910039	68095.892749	34.324416
1014.925074	68188.051522	34.329434
1015.891314	68300.503329	34.334452
1017.010354	68413.329471	34.339469
1018.101839	68511.801273	34.344487
1019.304441	68610.906590	34.349504
1020.328384	68691.486550	34.354522
1021.053629	68821.940162	34.359540
1022.652462	68897.988343	34.364557
1023.441378	69009.082613	34.369575
1024.873026	69088.095788	34.374592
1025.555221	69193.774994	34.379610
1026.754532	69294.893315	34.384628
1027.695689	69385.054198	34.389645
1028.732865	69488.865367	34.394663
1029.924798	69569.137943	34.399680
1030.803769	69696.199293	34.404698
1031.651105	69762.034570	34.409716
1033.119274	69875.287478	34.414733
1033.983629	69949.283288	34.419751
1035.095485	70060.913412	34.424768
1036.070460	70140.641610	34.429786
1036.946477	70254.976509	34.434804
1038.389382	70345.542171	34.439821
1039.341470	70435.314448	34.444839
1040.048556	70536.100510	34.449856
1041.259695	70583.122486	34.454874
1041.722633	70710.281870	34.459892
1043.045324	70772.121403	34.464909
1043.980726	70874.894675	34.469927
1045.190093	70959.201152	34.474944
1046.236056	71046.225531	34.479962
1047.217494	71145.903305	34.484980
1048.539674	71230.812188	34.489997
1049.243058	71315.699826	34.495015
1050.150486	71412.199996	34.500032
1051.249312	71491.364289	34.505050
1051.730708	71612.827435	34.510068
1053.015812	71697.851643	34.515085
1054.140213	71796.290518	34.520103
1055.089995	71902.699962	34.525120
1055.936589	72010.010982	34.530138
1057.024151	72118.042476	34.535156
1057.860323	72219.574840	34.540173
1058.466968	72349.950715	34.545191
1059.658514	72458.390872	34.550208
1060.858356	72555.513570	34.555226
1061.521518	72698.987667	34.560244
1063.400983	72807.143383	34.565261
1064.312681	72917.077559	34.570279
1065.840177	73027.407257	34.575296
1066.718832	73129.443028	34.580314
1068.021760	73226.565254	34.585332
1069.228300	73369.806107	34.590349
1070.174092	73447.277505	34.595367
1071.026375	73591.170282	34.600384
1072.307213	73684.197230	34.605402
1073.678135	73767.232500	34.610420
1074.720063	73913.182723	34.615437
1075.782634	74009.361223	34.620455
1077.048241	74102.095547	34.625472
1078.005872	74210.462407	34.630490
1078.960271	74319.418056	34.635508
1080.458626	74414.328538	34.640525
1081.012805	74525.661819	34.645543
1082.205233	74641.741119	34.650560
1083.360254	74747.261071	34.655578
1084.420169	74851.280052	34.660596
1085.499959	74958.519319	34.665613
1086.642241	75069.812632	34.670631
1087.913167	75180.574222	34.675648
1088.918217	75272.142071	34.680666
1089.922295	75385.557199	34.685684
1091.332475	75501.347738	34.690701
1092.400368	75582.277447	34.695719
1093.129274	75723.917465	34.700736
1094.642080	75807.065031	34.705754
1095.394610	75911.081514	34.710772
1096.323379	76031.312284	34.715789
1097.516058	76134.899687	34.720807
1098.590335	76220.431757	34.725824
1099.943454	76337.670781	34.730842
1100.766785	76433.816795	34.735860
1102.024485	76513.620395	34.740877
1102.853300	76616.288556	34.745895
1103.562989	76727.286957	34.750912
1104.945562	76812.323780	34.755930
1105.710340	76917.013413	34.760948
1106.849322	77041.002456	34.765965
1108.264300	77141.178418	34.770983
1109.264741	77244.922167	34.776000
1110.104815	77347.889290	34.781018
1111.024719	77471.852608	34.786036
1112.158900	77574.186321	34.791053
1112.920657	77686.610061	34.796071
1113.921711	77831.451192	34.801088
1115.549752	77932.324008	34.806106
1116.767120	78052.482943	34.811124
1117.741422	78148.417135	34.816141
1118.996846	78300.439064	34.821159
1120.361878	78419.723415	34.826176
1121.374492	78528.629302	34.831194
1122.130578	78650.969865	34.836212
1123.657543	78756.407332	34.841229
1124.918898	78879.787652	34.846247
1125.676725	79010.018252	34.851264
1127.019847	79114.469175	34.856282
1128.099895	79243.499641	34.861300
1129.027118	79368.933407	34.866317
1130.432761	79485.493248	34.871335
1131.790454	79610.537666	34.876352
1133.005081	79720.283719	34.881370
1133.938640	79864.568450	34.886388
1135.033334	79975.207228	34.891405
1136.199138	80075.645815	34.896423
1137.496636	80213.598345	34.901440
1138.732808	80330.910534	34.906458
1140.110206	80439.819116	34.911476
1140.949663	80553.927644	34.916493
1142.149775	80683.953111	34.921511
1143.310683	80806.728850	34.926528
1144.439909	80925.053857	34.931546
1145.535502	81051.760628	34.936564
1146.953690	81168.738884	34.941581
1148.163355	81286.850884	34.946599
1149.047326	81407.063494	34.951616
1150.395910	81515.976008	34.956634
1151.528359	81638.160663	34.961652
1152.824234	81755.363970	34.966669
1154.113503	81867.164055	34.971687
1155.039970	81986.026766	34.976704
1156.407240	82092.037718	34.981722
1157.527975	82220.328030	34.986740
1158.872332	82324.055365	34.991757
1159.936368	82430.862227	34.996775
1161.006175	82529.557898	35.001792
1162.344973	82647.322041	35.006810
1163.461082	82741.339544	35.011828
1164.355414	82834.912279	35.016845
1165.073617	82937.901438	35.021863
1166.172988	83045.584568	35.026880
1167.654457	83144.224002	35.031898
1168.117978	83260.202597	35.036916
1169.477175	83363.230998	35.041933
1170.572088	83484.522069	35.046951
1171.489872	83613.030222	35.051968
1172.925323	83727.156196	35.056986
1174.267343	83850.117059	35.062004
1175.489044	83966.459470	35.067021
1176.606984	84080.113113	35.072039
1177.478826	84202.354204	35.077056
1179.106291	84318.336891	35.082074
1179.487201	84454.585543	35.087092
1181.124333	84568.310995	35.092109
1182.527130	84687.625400	35.097127
1183.360998	84834.122646	35.102144
1184.525822	84942.924165	35.107162
1185.846469	85076.232850	35.112180
1186.760683	85205.389855	35.117197
1188.339346	85329.428165	35.122215
1189.720977	85467.351439	35.127232
1191.112603	85583.979236	35.132250
1192.067091	85714.549220	35.137268
1193.506827	85837.986652	35.142285
1195.156006	85965.855387	35.147303
1196.076601	86092.247396	35.152320
1197.526841	86190.577274	35.157338
1198.699151	86311.707881	35.162356
1199.906631	86437.620043	35.167373
1200.814877	86553.134992	35.172391
1201.872248	86678.629839	35.177408
1203.161104	86816.545005	35.182426
1204.415998	86918.241551	35.187444
1205.290927	87070.084352	35.192461
1207.307657	87166.880667	35.197479
1208.155727	87327.955040	35.202496
1209.381447	87435.020753	35.207514
1210.658725	87565.278844	35.212532
1211.747235	87703.016591	35.217549
1213.198801	87783.559834	35.222567
1214.230942	87946.829073	35.227584
1215.895948	88041.257099	35.232602
1216.812921	88193.765128	35.237620
1218.078303	88281.017405	35.242637
1219.307678	88425.933503	35.247655
1220.476483	88536.637136	35.252672
1221.754786	88658.105636	35.257690
1222.730969	88809.299623	35.262708
1224.257444	88914.282356	35.267725
1225.762353	89021.083928	35.272743
1226.360045	89162.690622	35.277760
1228.214563	89225.955688	35.282778
1229.038735	89349.346820	35.287796
1229.766193	89475.972857	35.292813
1231.231070	89566.316263	35.297831
1232.204132	89703.825870	35.302848
1233.428585	89787.233177	35.307866
1234.625782	89937.900318	35.312884
1235.698820	90027.138015	35.317901
1236.748572	90187.499702	35.322919
1238.093580	90282.291973	35.327936
1239.329894	90439.862244	35.332954
1240.256658	90537.043070	35.337972
1241.759617	90679.837461	35.342989
1243.002479	90790.477596	35.348007
1244.123431	90940.670511	35.353024
1245.186777	91078.079580	35.358042
1246.842961	91187.738992	35.363060
1248.173860	91351.644100	35.368077
1249.730243	91461.213239	35.373095
1250.698058	91604.433952	35.378112
1251.933321	91743.407300	35.383130
1253.521154	91849.880714	35.388148
1254.634156	92020.301765	35.393165
1255.835892	92103.867012	35.398183
1257.188805	92258.048189	35.403200
1258.689548	92385.365054	35.408218
1259.785866	92508.231120	35.413236
1260.988128	92646.064328	35.418253
1262.506344	92781.577569	35.423271
1263.176021	92909.567200	35.428288
1264.879505	93036.899872	35.433306
1266.281718	93174.002530	35.438324
1267.521322	93319.000103	35.443341
1269.297366	93428.550451	35.448359
1270.166443	93594.329319	35.453376
1271.314091	93686.542807	35.458394
1272.941911	93846.504077	35.463412
1273.881813	93977.309528	35.468429
1276.018637	94081.056218	35.473447
1276.966707	94248.958990	35.478464
1278.211763	94333.955287	35.483482
1279.731488	94476.158094	35.488500
1280.777882	94598.328941	35.493517
1281.971562	94745.158488	35.498535
1283.391858	94846.511510	35.503552
1284.518936	95007.775208	35.508570
1286.049061	95102.204586	35.513588
1287.186760	95257.301097	35.518605
1288.196494	95347.981003	35.523623
1289.237139	95519.762476	35.528640
1290.544878	95644.079809	35.533658
1292.463983	95747.495671	35.538676
1293.110603	95929.843453	35.543693
1294.708190	96051.384277	35.548711
1296.058891	96142.215615	35.553728
1297.125912	96284.647382	35.558746
1298.587316	96372.805231	35.563764
1299.316155	96531.992427	35.568781
1300.932787	96632.835233	35.573799
1301.946678	96768.686954	35.578816
1303.053643	96881.580512	35.583834
1304.379329	96987.582516	35.588852
1305.229972	97152.024249	35.593869
1307.059021	97272.940228	35.598887
1308.214892	97401.428644	35.603904
1309.264794	97548.330992	35.608922
1310.484999	97667.764338	35.613940
1311.848587	97825.246559	35.618957
1313.250867	97951.326596	35.623975
1314.792480	98104.297153	35.628992
1315.797219	98231.941270	35.634010
1317.493059	98378.138978	35.639028
1318.613592	98520.759771	35.644045
1319.973483	98658.022877	35.649063
1321.361529	98803.955925	35.654080
1322.490298	98942.807471	35.659098
1324.062258	99098.810279	35.664116
1325.051302	99228.101043	35.669133
1326.519508	99400.413373	35.674151
1328.034193	99523.966239	35.679168
1329.378621	99708.308583	35.684186
1330.643784	99816.187120	35.689204
1332.132667	99985.710464	35.694221
1333.627185	100114.577902	35.699239
1335.002508	100266.425224	35.704256
1336.136614	100422.734405	35.709274
1337.677862	100545.168680	35.714292
1338.861629	100720.244054	35.719309
1340.848902	100824.747808	35.724327
1341.763065	101023.809820	35.729344
1342.964127	101146.775893	35.734362
1345.121273	101254.285280	35.739380
1345.998468	101459.949802	35.744397
1347.292085	101565.781992	35.749415
1349.162432	101716.573113	35.754432
1350.407356	101838.112249	35.759450
1351.796174	101998.244914	35.764468
1352.754967	102135.383707	35.769485
1354.369539	102270.698015	35.774503
1355.423986	102413.188894	35.779520
1357.091862	102551.267787	35.784538
1358.613257	102689.959242	35.789556
1359.802171	102851.369740	35.794573
1361.272136	102969.101445	35.799591
1362.482983	103123.910643	35.804608
1363.896752	103286.642523	35.809626
1365.386660	103399.583160	35.814644
1367.123175	103521.059257	35.819661
1368.437237	103693.953211	35.824679
1369.455749	103792.138296	35.829696
1370.811629	103890.580234	35.834714
1372.148710	104056.487243	35.839732
1373.217138	104163.809766	35.844749
1374.233021	104303.761786	35.849767
1375.957261	104458.865206	35.854784
1377.017540	104545.808253	35.859802
1378.595239	104714.592545	35.864820
1379.790549	104831.364748	35.869837
1381.204748	104994.987980	35.874855
1382.587241	105107.726077	35.879872
1383.837793	105270.731749	35.884890
1385.484034	105393.934149	35.889908
1386.870308	105535.030627	35.894925
1387.887273	105672.282058	35.899943
1389.100772	105845.745648	35.904960
1390.532175	105964.916009	35.909978
1391.988346	106113.997600	35.914996
1392.795786	106293.547344	35.920013
1395.055810	106416.568897	35.925031
1396.312970	106581.512701	35.930048
1397.704350	106717.533529	35.935066
1399.080472	106908.243453	35.940084
1400.391961	107042.272639	35.945101
1401.870484	107171.276332	35.950119
1403.503768	107360.246553	35.955136
1405.056383	107485.911225	35.960154
1406.337732	107662.611234	35.965172
1407.909507	107787.135243	35.970189
1409.358559	107966.494280	35.975207
1410.944938	108088.125202	35.980224
1412.604771	108230.251042	35.985242
1413.975243	108414.935942	35.990260
1415.099661	108550.566540	35.995277
1416.715769	108672.423531	36.000295
1418.275909	108818.486405	36.005312
1419.397557	109007.247046	36.010330
1420.963731	109131.848505	36.015348
1422.521804	109267.515470	36.020365
1423.601244	109448.526554	36.025383
1425.086676	109594.086966	36.030400
1426.447934	109735.414625	36.035418
1428.573762	109885.742321	36.040436
1429.618580	110079.700974	36.045453
1430.844856	110210.324356	36.050471
1432.572321	110334.526574	36.055488
1434.112952	110499.319145	36.060506
1435.393957	110645.462664	36.065524
1436.502415	110790.729332	36.070541
1438.227048	110939.760065	36.075559
1439.534676	111120.494081	36.080576
1440.914213	111260.359146	36.085594
1441.982376	111415.402785	36.090612
1443.853833	111595.772182	36.095629
1445.301009	111713.044070	36.100647
1446.594400	111872.156575	36.105664
1447.543365	112037.104121	36.110682
1449.367438	112146.462658	36.115700
1450.842761	112299.769698	36.120717
1451.686646	112427.211976	36.125735
1453.410216	112594.882361	36.130752
1454.843347	112732.987477	36.135770
1456.547696	112880.963369	36.140788
1457.824632	113041.674887	36.145805
1459.383156	113179.224490	36.150823
1460.645993	113324.215654	36.155840
1462.283623	113499.761733	36.160858
1463.879287	113618.873848	36.165876
1464.843069	113809.234695	36.170893
1466.204447	113933.728437	36.175911
1467.866283	114116.650012	36.180928
1469.343863	114258.833383	36.185946
1470.495426	114425.290225	36.190964
1471.986925	114593.466735	36.195981
1473.550436	114757.771213	36.200999
1475.322304	114925.759792	36.206016
1476.429574	115112.378929	36.211034
1478.239050	115240.777352	36.216052
1479.481183	115445.907797	36.221069
1481.045228	115587.888690	36.226087
1483.345951	115784.104388	36.231104
1484.199572	115938.615111	36.236122
1485.896562	116102.691889	36.241140
1487.045424	116275.340446	36.246157
1489.125188	116458.662124	36.251175
1490.638613	116597.060651	36.256192
1492.337433	116802.446069	36.261210
1493.872680	116924.552757	36.266228
1495.150071	117114.888698	36.271245
1496.847431	117258.826786	36.276263
1498.084925	117436.002346	36.281280
1500.057070	117582.108239	36.286298
1501.330949	117771.056719	36.291316
1503.055769	117916.849261	36.296333
1504.653311	118100.765881	36.301351
1506.521053	118239.313293	36.306368
1507.842285	118398.715884	36.311386
1509.465122	118572.260723	36.316404
1510.820374	118696.880136	36.321421
1512.219035	118897.517983	36.326439
1514.172162	119028.204761	36.331456
1515.195653	119194.358563	36.336474
1517.005812	119334.959856	36.341492
1518.396138	119536.572756	36.346509
1519.485596	119678.981032	36.351527
1521.177640	119825.289802	36.356544
1522.856226	120014.931256	36.361562
1524.232921	120179.103995	36.366580
1526.659106	120300.369644	36.371597
1527.335999	120500.241747	36.376615
1528.921996	120624.124577	36.381632
1530.473317	120747.329632	36.386650
1532.237699	120904.378658	36.391668
1533.507814	121044.448116	36.396685
1534.748013	121192.096468	36.401703
1536.557194	121327.180621	36.406720
1537.381943	121487.637233	36.411738
1538.885539	121623.252719	36.416756
1540.720863	121791.263463	36.421773
1542.016306	121946.962114	36.426791
1543.164734	122117.376416	36.431808
1545.036366	122266.386962	36.436826
1546.523948	122422.691152	36.441844
1547.894487	122599.076548	36.446861
1549.603198	122749.825512	36.451879
1551.058108	122906.796351	36.456896
1552.542152	123095.819721	36.461914
1554.387892	123270.031628	36.466932
1555.948622	123424.050315	36.471949
1557.201644	123614.545291	36.476967
1558.587826	123777.941041	36.481984
1559.855527	123942.521873	36.487002
1561.794103	124150.263987	36.492020
1563.369233	124298.091792	36.497037
1565.045604	124516.745857	36.502055
1566.684073	124663.425668	36.507072
1568.142633	124874.631536	36.512090
1570.352533	125023.261812	36.517108
1571.369395	125216.300982	36.522125
1573.266690	125382.817278	36.527143
1575.151422	125543.636627	36.532160
1576.628770	125743.256388	36.537178
1578.049382	125925.431805	36.542196
1579.422472	126086.728339	36.547213
1581.842980	126240.499958	36.552231
1583.585455	126441.146776	36.557248
1584.761117	126642.138461	36.562266
1586.531480	126773.342254	36.567284
1588.220935	126967.705798	36.572301
1589.351348	127151.227605	36.577319
1591.478385	127289.698963	36.582336
1592.646324	127506.228509	36.587354
1594.389375	127650.488416	36.592372
1595.821830	127850.966849	36.597389
1597.478669	127998.307863	36.602407
1599.413961	128192.109022	36.607424
1600.662911	128378.939205	36.612442
1602.831658	128538.134989	36.617460
1604.487669	128699.883415	36.622477
1606.050596	128878.179509	36.627495
1607.740437	129035.199310	36.632512
1609.292825	129224.571345	36.637530
1610.878418	129410.746966	36.642548
1612.414208	129544.788340	36.647565
1613.812690	129740.687270	36.652583
1615.548237	129896.767229	36.657600
1616.764628	130028.479976	36.662618
1618.600552	130171.319441	36.667636
1620.315363	130362.637102	36.672653
1621.308117	130490.016810	36.677671
1623.055992	130667.230844	36.682688
1624.240022	130831.359758	36.687706
1625.847243	130972.668698	36.692724
1627.245823	131177.952851	36.697741
1629.409596	131336.709402	36.702759
1631.092600	131502.714062	36.707776
1632.758248	131708.681831	36.712794
1634.038625	131854.620797	36.717812
1635.866262	132028.992803	36.722829
1637.342769	132211.808974	36.727847
1639.139918	132392.788966	36.732864
1640.728175	132564.364281	36.737882
1642.271383	132736.682644	36.742900
1643.938164	132929.393761	36.747917
1645.567263	133112.305542	36.752935
1647.285799	133273.766419	36.757952
1648.865153	133491.835517	36.762970
1650.587780	133641.590541	36.767988
1652.269180	133847.647384	36.773005
1654.077592	134003.219062	36.778023
1655.772882	134222.390328	36.783040
1657.782970	134377.387177	36.788058
1659.301370	134595.056242	36.793076
1660.841064	134746.404606	36.798093
1662.559184	134954.680965	36.803111
1664.468263	135132.112724	36.808128
1665.861129	135308.930654	36.813146
1667.808867	135520.836565	36.818164
1669.554103	135682.598212	36.823181
1671.231504	135892.015539	36.828199
1672.988639	136050.698230	36.833216
1674.692181	136265.207986	36.838234
1676.493677	136423.074696	36.843252
1678.251247	136615.922841	36.848269
1679.696202	136786.583111	36.853287
1681.464329	136994.498711	36.858304
1682.846848	137147.620616	36.863322
1684.977895	137373.538643	36.868340
1686.477016	137525.478189	36.873357
1688.259302	137747.424791	36.878375
1690.160639	137897.515623	36.883392
1692.067963	138111.727778	36.888410
1693.619376	138265.158171	36.893428
1694.837459	138476.073578	36.898445
1696.273821	138660.673084	36.903463
1698.228327	138822.761029	36.908480
1699.973033	139020.075073	36.913498
1701.295282	139251.813283	36.918516
1703.421341	139395.881842	36.923533
1704.854165	139613.893352	36.928551
1706.581051	139793.093132	36.933568
1708.280714	139935.457804	36.938586
1710.040970	140131.750236	36.943604
1711.684727	140291.931209	36.948621
1713.443050	140440.384772	36.953639
1715.178913	140637.165976	36.958656
1716.171966	140796.895355	36.963674
1718.286681	140946.131272	36.968692
1719.801989	141124.384090	36.973709
1721.337511	141360.705252	36.978727
1722.953238	141515.219416	36.983744
1725.232800	141713.733657	36.988762
1726.827740	141897.339401	36.993780
1728.765182	142058.104158	36.998797
1730.267618	142295.743288	37.003815
1731.935511	142446.426368	37.008832
1733.831180	142666.883278	37.013850
1735.553689	142839.688743	37.018868
1737.137103	143026.078793	37.023885
1738.451738	143239.597857	37.028903
1740.759168	143406.242606	37.033920
1742.546430	143640.462889	37.038938
1744.103825	143809.979314	37.043956
1746.323138	144026.566886	37.048973
1747.602338	144225.091548	37.053991
1749.952897	144384.319994	37.059008
1751.666029	144624.389976	37.064026
1753.007222	144807.216917	37.069044
1755.144932	145014.964522	37.074061
1756.792203	145186.236076	37.079079
1758.890377	145407.466332	37.084096
1760.098815	145593.703286	37.089114
1762.564962	145765.469101	37.094132
1763.962869	145995.903017	37.099149
1765.172734	146220.372916	37.104167
1767.241417	146415.794763	37.109184
1769.444220	146598.482726	37.114202
1771.431877	146795.200057	37.119220
1773.341345	147003.123888	37.124237
1775.431402	147168.226189	37.129255
1776.753535	147383.433079	37.134272
1778.391677	147565.252925	37.139290
1780.808691	147743.768415	37.144308
1782.421730	147977.351730	37.149325
1783.771410	148158.384140	37.154343
1785.720596	148339.918190	37.159360
1788.345119	148533.654981	37.164378
1789.540403	148771.912040	37.169396
1791.491816	148933.458054	37.174413
1793.464548	149101.834281	37.179431
1795.373289	149284.698512	37.184448
1797.082294	149525.795290	37.189466
1798.306076	149694.331567	37.194484
1800.903902	149858.188244	37.199501
1802.614240	150030.997272	37.204519
1803.838086	150208.207392	37.209536
1805.631707	150372.777518	37.214554
1807.153651	150556.268179	37.219572
1808.984367	150767.702607	37.224589
1810.149977	150933.351447	37.229607
1812.155750	151084.377299	37.234624
1813.923386	151289.739913	37.239642
1815.453588	151506.792335	37.244660
1817.490092	151649.854326	37.249677
1819.183617	151891.300768	37.254695
1820.910615	152046.698486	37.259712
1822.720168	152276.858674	37.264730
1824.284077	152464.727314	37.269748
1826.576541	152629.749435	37.274765
1828.226246	152867.660123	37.279783
1829.762099	153048.500121	37.284800
1832.201840	153225.723737	37.289818
1833.806415	153455.797904	37.294836
1835.789967	153668.367818	37.299853
1837.334259	153903.589465	37.304871
1839.207013	154114.696418	37.309888
1841.422554	154316.621558	37.314906
1843.136985	154508.902778	37.319924
1844.804406	154711.006065	37.324941
1846.616682	154922.064320	37.329959
1848.190691	155126.746100	37.334976
1850.624109	155320.921134	37.339994
1852.207134	155534.365268	37.345012
1854.428529	155758.803828	37.350029
1856.187214	155981.757762	37.355047
1858.068970	156228.695928	37.360064
1860.330948	156437.118321	37.365082
1861.645723	156623.934056	37.370100
1864.569341	156817.545353	37.375117
1866.512193	157029.838632	37.380135
1868.223502	157264.004753	37.385152
1870.063238	157435.842723	37.390170
1871.879657	157670.362652	37.395188
1874.201553	157849.835625	37.400205
1875.573673	158078.494571	37.405223
1877.174790	158279.919497	37.410240
1879.404564	158463.163646	37.415258
1880.949069	158699.534339	37.420276
1883.318231	158874.072451	37.425293
1885.399690	159124.512227	37.430311
1887.372270	159343.789343	37.435328
1889.395380	159527.528419	37.440346
1890.753600	159728.467706	37.445364
1892.848215	159939.296462	37.450381
1895.122439	160122.047738	37.455399
1896.756378	160312.002958	37.460416
1898.589904	160508.787985	37.465434
1900.718324	160716.407729	37.470452
1902.731795	160943.018056	37.475469
1904.481760	161167.198803	37.480487
1906.512854	161349.196111	37.485504
1908.154892	161527.730665	37.490522
1909.459819	161702.312267	37.495540
1911.782254	161859.042449	37.500557
1913.807676	162074.029113	37.505575
1915.274025	162258.099041	37.510592
1917.391460	162397.718477	37.515610
1919.252396	162629.195497	37.520628
1920.615564	162794.578864	37.525645
1923.231153	162992.445600	37.530663
1924.969809	163173.344559	37.535680
1926.692976	163399.483905	37.540698
1928.225780	163585.566533	37.545716
1930.322947	163787.273831	37.550733
1931.879609	164003.728785	37.555751
1933.908503	164181.657104	37.560768
1936.256024	164419.675877	37.565786
1938.341503	164615.073761	37.570804
1940.006200	164807.115173	37.575821
1942.222894	165028.011817	37.580839
1944.102282	165219.057433	37.585856
1946.760688	165404.958020	37.590874
1948.325677	165666.876655	37.595892
1950.559985	165818.450671	37.600909
1952.717118	166042.914084	37.605927
1954.432049	166234.295453	37.610944
1956.801596	166440.146857	37.615962
1958.404447	166631.230982	37.620980
1960.688023	166859.370082	37.625997
1962.885492	167031.057927	37.631015
1964.475215	167250.849742	37.636032
1966.992105	167469.176622	37.641050
1968.601822	167658.755576	37.646068
1971.191000	167831.044474	37.651085
1973.015477	168066.810542	37.656103
1974.601489	168248.316711	37.661120
1976.910440	168424.166196	37.666138
1978.769348	168680.579890	37.671156
1980.749033	168865.248255	37.676173
1982.856037	169044.684180	37.681191
1984.665073	169280.498299	37.686208
1986.735564	169434.586340	37.691226
1988.828597	169679.452395	37.696244
1990.514120	169859.605932	37.701261
1993.007155	170077.583781	37.706279
1994.721497	170273.805785	37.711296
1996.830053	170486.037491	37.716314
1998.898541	170664.586519	37.721332
2000.885944	170888.369928	37.726349
2003.010606	171053.986202	37.731367
2004.907662	171288.618983	37.736384
2007.216702	171461.438054	37.741402
2009.092070	171665.024120	37.746420
2011.409439	171888.101311	37.751437
2013.137697	172041.873519	37.756455
2014.313956	172224.186515	37.761472
2017.375494	172370.733609	37.766490
2019.113657	172543.178704	37.771508
2020.760809	172729.884505	37.776525
2022.940447	172886.658224	37.781543
2024.314914	173077.671193	37.786560
2026.569471	173251.534316	37.791578
2028.384313	173495.682008	37.796596
2030.155962	173671.691330	37.801613
2031.802512	173852.694030	37.806631
2034.174696	174041.206487	37.811648
2035.953271	174252.216987	37.816666
2038.491921	174426.052852	37.821684
2040.644137	174675.177790	37.826701
2042.266684	174851.736084	37.831719
2044.791993	175032.300222	37.836736
2047.076008	175267.745138	37.841754
2048.691602	175481.693048	37.846772
2050.647753	175671.357481	37.851789
2052.206520	175855.237505	37.856807
2054.465481	176069.796861	37.861824
2057.417152	176266.131338	37.866842
2059.220620	176520.740024	37.871860
2061.022606	176700.550985	37.876877
2063.545776	176888.646797	37.881895
2065.528223	177139.526456	37.886912
2067.511411	177309.136669	37.891930
2070.052143	177505.009440	37.896948
2071.835466	177758.093880	37.901965
2074.284652	177939.862826	37.906983
2076.765650	178120.130467	37.912000
2078.749823	178305.298762	37.917018
2080.610463	178550.852386	37.922036
2083.061332	178758.303224	37.927053
2085.362723	178929.924882	37.932071
2087.209193	179145.491810	37.937088
2089.249061	179354.089214	37.942106
2091.466761	179525.219091	37.947124
2093.593936	179765.167783	37.952141
2095.983256	179948.731186	37.957159
2097.766751	180132.480310	37.962176
2100.558501	180305.856778	37.967194
2102.119483	180531.473862	37.972212
2104.690881	180690.625957	37.977229
2107.074069	180913.640524	37.982247
2108.565284	181086.515975	37.987264
2111.260515	181255.991089	37.992282
2113.203015	181498.897036	37.997300
2115.132559	181694.936985	38.002317
2117.565462	181851.006804	38.007335
2119.738138	182034.499334	38.012352
2121.878890	182260.820172	38.017370
2123.688933	182408.007603	38.022388
2126.036992	182605.799692	38.027405
2128.012779	182819.765880	38.032423
2129.727159	182963.379572	38.037440
2132.299172	183088.840177	38.042458
2133.789456	183294.054586	38.047476
2135.090314	183456.032228	38.052493
2137.696346	183632.116097	38.057511
2139.247971	183845.253679	38.062528
2141.821240	183992.731399	38.067546
2143.626240	184229.469588	38.072564
2145.795392	184400.309250	38.077581
2147.860422	184564.123797	38.082599
2149.893423	184774.029966	38.087616
2151.785775	184976.879011	38.092634
2153.488125	185170.927584	38.097652
2155.907374	185371.791492	38.102669
2158.130438	185563.284801	38.107687
2160.335876	185785.273740	38.112704
2162.522030	185991.126152	38.117722
2164.603954	186207.515436	38.122740
2166.855075	186402.142099	38.127757
2169.038226	186620.801373	38.132775
2171.014607	186879.060196	38.137792
2173.403531	187094.021843	38.142810
2175.824129	187331.985678	38.147828
2177.882290	187525.607186	38.152845
2180.645714	187702.824089	38.157863
2182.379920	187956.838266	38.162880
2184.942404	188173.592059	38.167898
2187.435882	188355.600273	38.172916
2189.491354	188591.534678	38.177933
2191.976207	188824.699205	38.182951
2193.981886	189060.275865	38.187968
2195.910653	189240.067509	38.192986
2198.867770	189424.328641	38.198004
2200.908020	189681.120863	38.203021
2203.184953	189876.811323	38.208039
2205.098222	190089.628757	38.213056
2207.248517	190299.947618	38.218074
2209.986162	190512.192034	38.223092
2212.041571	190722.020191	38.228109
2215.291742	190898.461312	38.233127
2217.178004	191130.069678	38.238144
2219.574023	191360.481535	38.243162
2221.881363	191540.475650	38.248180
2223.990592	191748.091572	38.253197
2226.323349	191945.088792	38.258215
2228.158781	192135.706036	38.263232
2230.797992	192305.434220	38.268250
2232.968593	192516.762133	38.273268
2234.854154	192766.640732	38.278285
2237.132956	192964.145581	38.283303
2239.353261	193174.402398	38.288320
2241.581888	193358.413425	38.293338
2244.034808	193537.541520	38.298356
2246.306101	193729.238048	38.303373
2248.385815	193923.668952	38.308391
2250.378541	194137.900270	38.313408
2252.395958	194349.006501	38.318426
2254.306680	194513.273596	38.323444
2256.000737	194697.082455	38.328461
2258.881682	194896.720528	38.333479
2260.673146	195099.260867	38.338496
2262.839394	195278.732587	38.343514
2264.860225	195499.907606	38.348532
2266.670428	195697.218379	38.353549
2268.902457	195915.391842	38.358567
2270.658763	196145.889345	38.363584
2272.956001	196359.383753	38.368602
2275.296847	196577.225489	38.373620
2277.555926	196809.435819	38.378637
2279.781405	197024.124730	38.383655
2281.669215	197268.555032	38.388672
2284.222797	197493.081054	38.393690
2286.952989	197720.334264	38.398708
2289.179288	197980.731884	38.403725
2291.521763	198212.122956	38.408743
2293.791406	198418.179793	38.413760
2296.194583	198703.442827	38.418778
2298.689058	198948.216321	38.423796
2300.787470	199167.922361	38.428813
2303.662083	199384.891541	38.433831
2305.622811	199645.809112	38.438848
2308.039707	199929.312262	38.443866
2310.698592	200172.580252	38.448884
2312.652690	200413.194040	38.453901
2314.849541	200660.980014	38.458919
2317.415036	200905.827352	38.463936
2319.694805	201120.283092	38.468954
2322.739511	201338.032841	38.473972
2325.046920	201589.854623	38.478989
2327.481321	201825.600474	38.484007
2329.216400	202096.986756	38.489024
2331.204263	202340.446976	38.494042
2334.108128	202577.035521	38.499060
2337.009505	202820.606876	38.504077
2339.504474	203057.744650	38.509095
2341.562430	203300.525196	38.514112
2343.788138	203573.249860	38.519130
2346.268945	203807.752769	38.524148
2348.523538	204034.346236	38.529165
2351.355461	204282.098482	38.534183
2353.446547	204549.111591	38.539200
2355.235059	204767.505479	38.544218
2358.515672	204993.546577	38.549236
2360.390168	205273.659475	38.554253
2362.720930	205478.679462	38.559271
2365.029116	205722.331922	38.564288
2367.506083	206003.774570	38.569306
2370.161714	206217.707748	38.574324
2372.068114	206493.987807	38.579341
2374.824704	206695.288612	38.584359
2377.197463	206912.468138	38.589376
2379.402847	207169.586249	38.594394
2381.513979	207344.003259	38.599412
2383.573236	207598.937557	38.604429
2385.376523	207803.071800	38.609447
2387.846433	208031.004994	38.614464
2389.816830	208286.756064	38.619482
2392.244368	208502.993288	38.624500
2394.379411	208786.699505	38.629517
2396.820403	208999.508781	38.634535
2399.811414	209220.965667	38.639552
2401.795051	209504.927733	38.644570
2404.056894	209779.985917	38.649588
2406.354803	210015.418450	38.654605
2409.455730	210237.077388	38.659623
2411.378661	210543.447937	38.664640
2413.466355	210782.839493	38.669658
2416.611426	211022.013567	38.674676
2418.577242	211319.050118	38.679693
2420.836903	211579.796300	38.684711
2422.803747	211841.719859	38.689728
2425.642580	212110.158677	38.694746
2428.272097	212399.757102	38.699764
2430.896322	212666.911939	38.704781
2432.944414	212949.343147	38.709799
2435.669515	213207.800436	38.714816
2438.253020	213517.559161	38.719834
2440.983202	213744.799024	38.724852
2443.175139	214062.011319	38.729869
2445.850976	214308.787914	38.734887
2448.537552	214587.379690	38.739904
2450.754958	214881.167900	38.744922
2453.390258	215132.245213	38.749940
2456.042026	215426.411324	38.754957
2459.047881	215694.787540	38.759975
2461.227640	215963.600466	38.764992
2463.601740	216252.253245	38.770010
2466.202933	216503.658451	38.775028
2468.395663	216810.993159	38.780045
2471.310479	217057.500678	38.785063
2473.547772	217331.121757	38.790080
2475.775038	217635.585246	38.795098
2478.508121	217882.086398	38.800116
2480.646430	218189.892877	38.805133
2483.647171	218448.186800	38.810151
2485.959886	218736.326327	38.815168
2488.581746	219007.620246	38.820186
2491.470894	219279.368003	38.825204
2493.791031	219560.221711	38.830221
2496.264835	219822.222693	38.835239
2498.520854	220116.788636	38.840256
2501.091529	220382.458382	38.845274
2503.629869	220685.971316	38.850292
2506.622620	220944.707108	38.855309
2508.876245	221208.881030	38.860327
2511.494018	221445.292994	38.865344
2513.646405	221712.671722	38.870362
2515.833955	221993.568383	38.875380
2517.827047	222259.780749	38.880397
2520.127384	222513.362302	38.885415
2522.778593	222764.959090	38.890432
2524.900294	223034.213832	38.895450
2527.548644	223297.151599	38.900468
2529.803099	223570.615418	38.905485
2532.155969	223853.473478	38.910503
2534.667305	224123.990782	38.915520
2536.983955	224431.921701	38.920538
2539.684416	224696.760543	38.925556
2541.956613	224982.974911	38.930573
2544.821356	225275.432585	38.935591
2547.575142	225571.400801	38.940608
2549.986215	225852.047296	38.945626
2553.038654	226156.744536	38.950644
2555.287031	226450.713572	38.955661
2558.102231	226748.187365	38.960679
2560.436096	227044.417900	38.965696
2563.123970	227341.558441	38.970714
2565.861076	227628.457535	38.975732
2568.424726	227941.771895	38.980749
2571.163980	228242.437546	38.985767
2573.545890	228539.249811	38.990784
2576.009987	228840.773842	38.995802
2579.114059	229146.184794	39.000820
2581.492764	229456.816508	39.005837
2584.204143	229757.085468	39.010855
2586.697723	230070.418602	39.015872
2589.421286	230384.224335	39.020890
2591.947358	230687.802009	39.025908
2594.637360	230996.459570	39.030925
2597.351245	231305.215982	39.035943
2600.193382	231621.953294	39.040960
2602.544384	231928.356541	39.045978
2605.478090	232229.487365	39.050996
2608.186685	232536.623273	39.056013
2610.817115	232854.922171	39.061031
2613.572984	233149.277516	39.066048
2616.013376	233458.566917	39.071066
2619.027011	233765.150493	39.076084
2621.363932	234075.321790	39.081101
2623.735218	234384.675885	39.086119
2626.543573	234689.821791	39.091136
2629.156832	235012.244988	39.096154
2631.569565	235314.585481	39.101172
2634.476110	235630.411414	39.106189
2637.054866	235936.689619	39.111207
2639.825325	236238.519010	39.116224
2642.046809	236565.606349	39.121242
2644.960233	236880.114299	39.126260
2647.894974	237182.402978	39.131277
2650.324622	237492.747799	39.136295
2652.955649	237764.023399	39.141312
2655.375764	238044.629145	39.146330
2657.807443	238315.277341	39.151348
2660.352110	238614.609362	39.156365
2662.921145	238895.828686	39.161383
2665.780127	239183.022424	39.166400
2667.591552	239484.581100	39.171418
2670.627110	239761.664803	39.176436
2673.523709	240072.679518	39.181453
2675.641993	240371.575791	39.186471
2678.379052	240676.572321	39.191488
2680.616142	240994.170904	39.196506
2683.265721	241300.732303	39.201524
2685.802314	241618.691517	39.206541
2688.292881	241950.882809	39.211559
2691.289378	242275.400279	39.216576
2693.770665	242608.077440	39.221594
2696.890329	242930.418132	39.226612
2699.420865	243275.459134	39.231629
2702.048697	243609.944571	39.236647
2704.791964	243934.506485	39.241664
2707.717565	244280.833853	39.246682
2710.620000	244609.893519	39.251700
2713.623268	244954.305341	39.256717
2716.252402	245291.639764	39.261735
2719.218291	245619.802869	39.266752
2721.564869	245981.263568	39.271770
2724.729770	246302.310000	39.276788
2727.437896	246651.497426	39.281805
2729.756502	246985.608498	39.286823
2733.065778	247328.733174	39.291840
2735.830764	247682.003678	39.296858
2738.546482	248020.677236	39.301876
2741.317681	248364.092793	39.306893
2744.102838	248708.319768	39.311911
2747.314038	249046.282147	39.316928
2750.132700	249404.298259	39.321946
2752.822580	249730.101292	39.326964
2755.688989	250069.695400	39.331981
2758.125945	250422.109779	39.336999
2761.134684	250761.809818	39.342016
2763.400138	251107.419843	39.347034
2766.501491	251445.709540	39.352052
2768.915994	251800.594380	39.357069
2771.836490	252146.280603	39.362087
2775.040959	252509.246542	39.367104
2777.378925	252857.236389	39.372122
2780.538872	253213.504745	39.377140
2783.244689	253556.763742	39.382157
2785.723374	253894.267706	39.387175
2788.628260	254252.940852	39.392192
2791.457142	254610.000981	39.397210
2793.896550	254964.761056	39.402228
2796.778150	255311.500869	39.407245
2799.449674	255669.121287	39.412263
2802.449409	255990.822409	39.417280
2804.973081	256313.869539	39.422298
2807.839004	256638.488712	39.427316
2810.225720	256974.183481	39.432333
2812.681203	257298.894049	39.437351
2815.465308	257629.598826	39.442368
2818.085710	257973.386873	39.447386
2821.129229	258323.179624	39.452404
2823.822596	258662.867335	39.457421
2826.209996	259019.242662	39.462439
2829.653383	259353.630448	39.467456
2832.446571	259716.775821	39.472474
2835.110397	260064.700592	39.477492
2837.827173	260421.889430	39.482509
2840.355008	260785.967404	39.487527
2843.704752	261150.271349	39.492544
2846.045794	261514.938721	39.497562
2848.831896	261879.993329	39.502580
2851.983308	262263.763261	39.507597
2854.464979	262653.202966	39.512615
2857.551987	263021.589884	39.517632
2860.594821	263403.244563	39.522650
2863.167564	263793.153879	39.527668
2866.185257	264173.086007	39.532685
2869.126678	264554.249966	39.537703
2872.013064	264950.741086	39.542720
2874.991059	265353.619695	39.547738
2877.937930	265738.721459	39.552756
2880.983978	266128.761494	39.557773
2883.776624	266525.726266	39.562791
2887.203216	266921.676501	39.567808
2890.149734	267312.749461	39.572826
2893.088213	267700.470782	39.577844
2896.331533	268093.021555	39.582861
2898.855738	268482.536468	39.587879
2902.082609	268863.328684	39.592896
2904.905800	269258.512516	39.597914
2907.972455	269644.589065	39.602932
2911.344944	270029.042408	39.607949
2913.814482	270427.407525	39.612967
2917.170024	270805.868764	39.617984
2920.085793	271197.050676	39.623002
2922.721182	271579.614596	39.628020
2926.133839	271968.863712	39.633037
2928.932699	272368.574726	39.638055
2931.911084	272746.004072	39.643072
2934.623357	273133.205154	39.648090
2937.581089	273509.596425	39.653108
2940.431400	273909.325110	39.658125
2942.975784	274308.416405	39.663143
2946.127727	274711.831763	39.668160
2949.012870	275100.377590	39.673178
2951.421868	275495.248060	39.678196
2954.916845	275899.853948	39.683213
2957.870742	276296.543410	39.688231
2960.915625	276642.462416	39.693248
2963.573121	277004.726310	39.698266
2966.509958	277378.758526	39.703284
2969.375286	277737.331330	39.708301
2972.308921	278102.650562	39.713319
2975.109193	278462.986357	39.718336
2977.956347	278838.124819	39.723354
2980.442966	279217.003734	39.728372
2982.951338	279591.789138	39.733389
2985.804387	279987.680845	39.738407
2989.175570	280382.245604	39.743424
2991.691568	280783.296390	39.748442
2994.784064	281189.742836	39.753460
2997.765386	281591.989708	39.758477
3000.507722	282014.673019	39.763495
3003.517605	282418.921731	39.768512
3006.630087	282831.206765	39.773530
3009.573268	283260.995728	39.778548
3012.713995	283661.386959	39.783565
3015.576973	284096.471800	39.788583
3018.939146	284520.909516	39.793600
3022.036240	284950.825073	39.798618
3024.964375	285395.195927	39.803636
3028.108566	285819.717699	39.808653
3031.014494	286266.021760	39.813671
3034.286481	286693.113475	39.818688
3037.525147	287116.348714	39.823706
3040.223519	287568.780777	39.828724
3043.757381	288012.087364	39.833741
3046.726261	288455.609794	39.838759
3049.972841	288885.497119	39.843776
3053.128242	289327.794861	39.848794
3056.439228	289771.185046	39.853812
3059.756480	290198.950865	39.858829
3062.992606	290638.922178	39.863847
3066.101347	291062.858449	39.868864
3069.312641	291496.862659	39.873882
3072.213962	291921.541639	39.878900
3075.716797	292353.085003	39.883917
3078.714873	292786.714286	39.888935
3081.911415	293227.271644	39.893952
3085.116623	293656.700542	39.898970
3088.035017	294082.998723	39.903988
3091.310019	294512.770569	39.909005
3094.217070	294945.825879	39.914023
3097.157081	295382.914036	39.919040
3100.714952	295812.917902	39.924058
3103.450200	296264.185578	39.929076
3106.544540	296700.179581	39.934093
3109.525803	297132.837437	39.939111
3113.170409	297555.990625	39.944128
3116.096099	297994.777157	39.949146
3118.932314	298428.902863	39.954164
3122.689057	298865.498228	39.959181
3125.205650	299292.305897	39.964199
3128.113995	299693.267882	39.969216
3131.381231	300090.641314	39.974234
3134.327667	300489.868070	39.979252
3137.022927	300900.716654	39.984269
3140.259329	301299.412917	39.989287
3142.586921	301703.586261	39.994304
3145.676631	302131.134109	39.999322
3148.520662	302556.941564	40.004340
3151.933840	302977.120329	40.009357
3154.541953	303415.307614	40.014375
3157.624879	303856.085561	40.019392
3160.904356	304296.221444	40.024410
3164.056763	304749.152666	40.029428
3167.355258	305187.047498	40.034445
3170.276656	305652.433273	40.039463
3173.611957	306101.241624	40.044480
3176.982791	306548.366421	40.049498
3180.046263	307030.108213	40.054516
3183.558493	307470.095397	40.059533
3186.329421	307936.512937	40.064551
3189.520719	308412.971473	40.069568
3192.978808	308873.333192	40.074586
3196.457301	309358.708837	40.079604
3199.489214	309823.172977	40.084621
3202.643908	310297.928154	40.089639
3206.062788	310775.611369	40.094656
3209.222727	311248.939479	40.099674
3212.613516	311742.497801	40.104692
3216.444792	312211.397807	40.109709
3219.258705	312686.527192	40.114727
3222.439361	313171.603725	40.119744
3225.840687	313645.975638	40.124762
3229.110903	314133.548176	40.129780
3232.380620	314603.822046	40.134797
3235.581363	315097.217414	40.139815
3239.286357	315570.389687	40.144832
3242.397078	316056.225956	40.149850
3244.922559	316552.895910	40.154868
3248.742214	317037.116785	40.159885
3252.126938	317528.312328	40.164903
3255.561166	318021.148421	40.169920
3258.993316	318510.375848	40.174938
3262.142254	318996.750239	40.179956
3265.525368	319476.507138	40.184973
3268.979665	319976.491950	40.189991
3272.071650	320439.781666	40.195008
3275.633932	320940.125090	40.200026
3278.996853	321419.036902	40.205044
3282.467349	321899.427531	40.210061
3285.364087	322387.449095	40.215079
3288.776210	322868.732532	40.220096
3292.177611	323362.636956	40.225114
3295.192053	323840.777915	40.230132
3298.764879	324319.234187	40.235149
3301.725972	324803.168417	40.240167
3304.837244	325262.924717	40.245184
3308.051205	325703.971037	40.250202
3310.790132	326158.473518	40.255220
3314.205381	326596.537273	40.260237
3317.110174	327062.182353	40.265255
3320.494991	327518.378009	40.270272
3323.919776	327976.266153	40.275290
3326.719416	328457.892978	40.280308
3330.178005	328926.308979	40.285325
3333.205091	329411.779223	40.290343
3336.323116	329883.188957	40.295360
3339.851899	330376.166533	40.300378
3342.916261	330873.912173	40.305396
3346.007639	331365.352537	40.310413
3349.519675	331865.915544	40.315431
3352.743710	332376.881148	40.320448
3356.370149	332888.896780	40.325466
3359.473514	333402.845147	40.330484
3363.121784	333911.574242	40.335501
3366.534666	334438.822715	40.340519
3369.795949	334953.014039	40.345536
3373.445065	335464.677132	40.350554
3376.729976	335999.830865	40.355572
3380.400071	336512.650773	40.360589
3383.764950	337032.370775	40.365607
3386.913274	337577.156950	40.370624
3390.864856	338097.689888	40.375642
3393.965210	338623.152199	40.380660
3397.583078	339151.829217	40.385677
3401.069030	339680.903600	40.390695
3404.224586	340223.558932	40.395712
3408.112937	340757.841902	40.400730
3411.384691	341301.129701	40.405748
3415.097916	341831.114867	40.410765
3418.534911	342372.945292	40.415783
3422.084377	342903.988053	40.420800
3425.953985	343432.335071	40.425818
3429.244789	343975.723017	40.430836
3432.869150	344495.467218	40.435853
3436.352811	345033.889593	40.440871
3439.388280	345576.490787	40.445888
3443.234396	346101.669556	40.450906
3446.662341	346640.796759	40.455924
3450.036042	347183.126297	40.460941
3453.673427	347721.093150	40.465959
3457.135022	348251.745837	40.470976
3460.621755	348784.648952	40.475994
3463.847582	349329.266016	40.481012
3467.572390	349867.274555	40.486029
3470.736950	350408.895056	40.491047
3474.404545	350945.962748	40.496064
3477.811088	351486.772666	40.501082
3481.041117	352013.135457	40.506100
3484.318240	352578.197717	40.511117
3488.221100	353081.957125	40.516122
3491.340451	353586.230113	40.521127
3494.470802	354029.240310	40.526132
3497.184728	354431.925017	40.531136
3500.012971	354759.743529	40.536141
3502.721523	355050.449243	40.541146
3504.483549	355285.137968	40.546151
3506.468219	355482.966478	40.551156
3507.876060	355684.346394	40.556160
3509.436325	355793.374974	40.561165
3511.122467	355884.925902	40.566170
3512.060704	355952.597215	40.571175
3513.214671	355998.908725	40.576180
3514.066387	355996.127481	40.581184
3515.013471	355975.466503	40.586189
3515.470266	355943.685798	40.591194
3515.835898	355898.228317	40.596199
3516.292693	355800.943628	40.601204
3516.188701	355721.866644	40.606208
3516.457834	355641.839856	40.611213
3516.894982	355527.710907	40.616218
3516.570600	355404.616974	40.621223
3516.601690	355309.841706	40.626228
3516.475812	355185.188949	40.631232
3516.572411	355039.658236	40.636237
3516.277805	354938.851533	40.641242
3516.292863	354806.006525	40.646247
3516.261173	354657.695642	40.651252
3515.727212	354532.164208	40.656256
3515.541722	354406.501031	40.661261
3515.402546	354266.095211	40.666266
3515.038040	354140.815978	40.671271
3514.927017	354013.816721	40.676276
3514.432197	353885.681714	40.681280
3514.786917	353759.117191	40.686285
3514.380262	353635.344915	40.691290
3513.925913	353516.440731	40.696295
3514.146356	353394.910095	40.701300
3513.686122	353276.108094	40.706304
3513.476490	353150.496605	40.711309
3513.102473	353031.451373	40.716314
3512.601637	352916.854177	40.721319
3512.370293	352815.957013	40.726324
3511.856921	352714.060800	40.731328
3511.929335	352612.733478	40.736333
3511.557411	352502.492382	40.741338
3511.497937	352435.339378	40.746343
3511.564094	352329.635109	40.751348
3511.084948	352233.204315	40.756352
3510.791908	352152.726592	40.761357
3510.851325	352057.864593	40.766362
3510.480216	351981.038324	40.771367
3510.252170	351895.307199	40.776372
3510.175072	351820.215733	40.781376
3510.113546	351741.685910	40.786381
3510.207428	351673.336987	40.791386
3509.198337	351584.980208	40.796391
3509.544924	351519.848786	40.801396
3509.294476	351454.837124	40.806400
3508.789836	351400.198459	40.811405
3509.017853	351354.733337	40.816410
3508.733759	351292.831757	40.821415
3508.726035	351226.636173	40.826420
3508.434042	351172.294515	40.831424
3508.425389	351115.693806	40.836429
3508.768518	351050.129703	40.841434
3508.386049	350997.456464	40.846439
3508.448165	350944.483830	40.851444
3508.465712	350906.763160	40.856448
3507.962039	350850.036828	40.861453
3507.917451	350800.644024	40.866458
3507.639616	350765.794987	40.871463
3507.881129	350711.215816	40.876468
3507.833681	350666.786246	40.881472
3507.390071	350621.095828	40.886477
3507.736640	350575.509505	40.891482
3507.083142	350535.425934	40.896487
3507.341321	350495.274553	40.901492
3507.102963	350458.561162	40.906496
3506.824736	350423.050244	40.911501
3507.013265	350400.878153	40.916506
3506.672333	350364.639032	40.921511
3507.038444	350331.011360	40.926516
3506.482807	350309.567705	40.931520
3506.569544	350272.828244	40.936525
3506.876077	350243.180292	40.941530
3506.656239	350217.458645	40.946535
3506.913597	350182.957289	40.951540
3506.810813	350162.536376	40.956544
3506.662769	350123.772399	40.961549
3506.444304	350104.158736	40.966554
3506.455812	350069.288960	40.971559
3506.800521	350042.892602	40.976564
3506.232947	350026.311883	40.981568
3506.270630	349993.983031	40.986573
3506.512030	349963.505338	40.991578
3506.212017	349945.889699	40.996583
3506.404195	349927.636316	41.001588
3506.162520	349912.327498	41.006592
3506.234890	349880.349412	41.011597
3506.301367	349854.149658	41.016602
3505.826670	349832.896629	41.021607
3506.339701	349811.589240	41.026612
3505.928070	349784.217931	41.031616
3505.883557	349771.244867	41.036621
3506.289596	349752.066821	41.041626
3506.187123	349732.434687	41.046631
3506.014467	349701.360577	41.051636
3505.718861	349681.478994	41.056640
3505.990059	349653.719704	41.061645
3505.731125	349645.667154	41.066650
3505.582417	349636.884541	41.071655
3506.118985	349606.996267	41.076660
3506.009616	349604.112131	41.081664
3505.873731	349565.193129	41.086669
3505.897491	349550.809396	41.091674
3505.718649	349532.258220	41.096679
3505.955209	349516.670074	41.101684
3505.704549	349497.341249	41.106688
3505.959033	349464.672394	41.111693
3505.830214	349448.429356	41.116698
3505.612216	349438.817770	41.121703
3505.936227	349428.662368	41.126708
3505.761752	349411.052162	41.131712
3505.792682	349383.916104	41.136717
3505.647637	349362.025393	41.141722
3505.606635	349351.291399	41.146727
3505.773688	349317.567321	41.151732
3505.454775	349314.105463	41.156736
3505.609492	349299.700961	41.161741
3505.381992	349286.222232	41.166746
3505.517728	349277.903621	41.171751
3505.635299	349250.499285	41.176756
3505.608844	349235.359865	41.181760
3505.518067	349222.572145	41.186765
3505.838257	349201.829490	41.191770
3505.736822	349181.255291	41.196775
3505.936566	349162.873201	41.201780
3505.381083	349146.875689	41.206784
3505.512872	349129.420585	41.211789
3505.667358	349122.295208	41.216794
3505.201210	349103.840214	41.221799
3505.616691	349082.318903	41.226804
3505.549693	349087.038051	41.231808
3505.317684	349071.574762	41.236813
3505.282368	349048.444905	41.241818
3505.429195	349030.249298	41.246823
3505.309187	349014.513771	41.251828
3505.522955	349007.633522	41.256832
3505.591979	349008.437081	41.261837
3505.765831	348975.118946	41.266842
3505.282523	348963.767611	41.271847
3505.837687	348940.340743	41.276852
3505.455270	348914.058804	41.281856
3505.343958	348908.451615	41.286861
3505.479101	348901.660139	41.291866
3505.171217	348897.865640	41.296871
3505.420405	348866.291691	41.301876
3504.989686	348861.549447	41.306880
3505.100971	348868.861947	41.311885
3505.246850	348843.285453	41.316890
3505.091474	348834.529218	41.321895
3505.197581	348805.599376	41.326900
3505.247270	348810.503713	41.331904
3505.433815	348791.334586	41.336909
3505.663041	348783.077475	41.341914
3505.255150	348771.459661	41.346919
3505.584250	348743.512599	41.351924
3505.051471	348732.169038	41.356928
3505.282197	348715.970749	41.361933
3505.449012	348702.760410	41.366938
3504.997481	348699.319480	41.371943
3505.283683	348692.911324	41.376948
3505.007175	348672.440970	41.381952
3504.829606	348662.670148	41.386957
3505.024428	348671.267505	41.391962
3504.777630	348651.759612	41.396967
3505.358189	348645.279462	41.401972
3505.392001	348639.598398	41.406976
3505.236832	348627.380661	41.411981
3505.468289	348603.775764	41.416986
3505.211474	348597.555253	41.421991
3505.463230	348574.685236	41.426996
3505.391703	348562.963296	41.432000
3505.096095	348548.757054	41.437005
3505.379912	348533.364775	41.442010
3505.021562	348526.676725	41.447015
3505.245480	348503.785628	41.452020
3505.025993	348500.842488	41.457024
3504.885387	348489.233262	41.462029
3504.999672	348483.183135	41.467034
3504.859620	348473.253637	41.472039
3504.927003	348465.836525	41.477044
3504.960580	348468.070998	41.482048
3504.995593	348429.709574	41.487053
3504.902982	348449.932994	41.492058
3505.180404	348428.484162	41.497063
3505.184395	348406.264091	41.502068
3505.050385	348407.965121	41.507072
3505.011092	348392.751145	41.512077
3505.256558	348402.714938	41.517082
3505.038276	348366.455116	41.522087
3505.132886	348360.611701	41.527092
3505.269967	348337.657909	41.532096
3505.019590	348328.611192	41.537101
3504.874691	348332.324645	41.542106
3504.798340	348313.425984	41.547111
3505.181374	348302.013903	41.552116
3504.879622	348301.527140	41.557120
3504.903458	348288.288404	41.562125
3504.921607	348289.965382	41.567130
3504.751525	348287.116227	41.572135
3505.056280	348263.932281	41.577140
3504.664780	348268.422831	41.582144
3504.865457	348261.849983	41.587149
3504.985474	348256.562483	41.592154
3504.807402	348247.555225	41.597159
3505.048760	348222.803266	41.602164
3505.080612	348211.904823	41.607168
3504.709361	348217.206637	41.612173
3504.926484	348200.832186	41.617178
3504.926134	348200.934070	41.622183
3504.968679	348185.172610	41.627188
3504.738046	348195.338969	41.632192
3504.627043	348170.999022	41.637197
3504.923145	348165.963646	41.642202
3504.674802	348156.356636	41.647207
3504.810809	348152.033773	41.652212
3504.949364	348159.596574	41.657216
3504.493889	348152.058467	41.662221
3504.825360	348127.444931	41.667226
3504.679232	348123.573902	41.672231
3505.067684	348134.813188	41.677236
3505.065711	348116.589904	41.682240
3504.820903	348107.924051	41.687245
3504.966360	348098.102060	41.692250
3504.694904	348085.724425	41.697255
3504.798388	348075.883615	41.702260
3504.683364	348073.382073	41.707264
3504.686022	348063.888076	41.712269
3505.023144	348054.646624	41.717274
3504.807100	348056.564250	41.722279
3505.024135	348038.433577	41.727284
3504.989203	348047.474586	41.732288
3504.987479	348029.505756	41.737293
3505.003787	348003.109447	41.742298
3504.724883	348012.723526	41.747303
3505.135456	347988.555560	41.752308
3505.144791	347982.801944	41.757312
3504.600522	347971.867277	41.762317
3504.699518	347956.860390	41.767322
3504.588130	347957.667035	41.772327
3505.092309	347951.020716	41.777332
3504.589999	347947.053274	41.782336
3504.726170	347938.072641	41.787341
3504.823119	347933.094183	41.792346
3504.431311	347926.716775	41.797351
3504.855482	347930.442094	41.802356
3505.068190	347927.685115	41.807360
3505.004365	347913.111190	41.812365
3504.881917	347909.261855	41.817370
3504.877532	347903.510400	41.822375
3505.011976	347879.513303	41.827380
3504.584817	347870.010871	41.832384
3504.687091	347869.562037	41.837389
3505.266879	347856.057140	41.842394
3504.780203	347849.185680	41.847399
3505.053903	347834.634730	41.852404
3504.828921	347823.013253	41.857408
3504.764536	347819.994652	41.862413
3504.920931	347813.123327	41.867418
3504.729951	347807.299555	41.872423
3504.591131	347787.316152	41.877428
3504.598630	347795.052435	41.882432
3504.656878	347788.247528	41.887437
3504.874223	347775.945260	41.892442
3504.574554	347779.861382	41.897447
3504.589664	347768.507362	41.902452
3504.756149	347764.612337	41.907456
3504.604228	347751.884853	41.912461
3504.627172	347750.074144	41.917466
3504.592959	347753.617422	41.922471
3504.872692	347741.890682	41.927476
3504.688238	347729.957353	41.932480
3504.600161	347733.865479	41.937485
3504.848613	347722.296393	41.942490
3504.360066	347714.483482	41.947495
3504.689940	347697.327495	41.952500
3504.409120	347690.321661	41.957504
3504.166221	347707.107612	41.962509
3504.417258	347706.737066	41.967514
3504.536065	347703.282262	41.972519
3504.459362	347684.917941	41.977524
3504.898855	347692.509584	41.982528
3504.820358	347683.791919	41.987533
3504.771802	347666.237612	41.992538
3504.603208	347664.915322	41.997543
3504.731791	347656.724862	42.002548
3504.308768	347663.002096	42.007552
3504.535114	347662.253671	42.012557
3504.441112	347629.791554	42.017562
3504.109622	347637.835974	42.022567
3504.448823	347640.556658	42.027572
3504.302244	347651.855174	42.032576
3504.685460	347642.682725	42.037581
3504.410095	347638.119433	42.042586
3504.561063	347639.470005	42.047591
3504.716572	347628.271925	42.052596
3504.653212	347628.740103	42.057600
3504.904031	347633.740006	42.062605
3504.730320	347611.827690	42.067610
3504.381777	347611.068344	42.072615
3504.378939	347600.455242	42.077620
3504.307499	347610.647442	42.082624
3504.538641	347598.851998	42.087629
3505.018989	347579.814174	42.092634
3504.567380	347596.022301	42.097639
3504.753376	347586.499239	42.102644
3504.608118	347581.940825	42.107648
3504.606494	347563.819117	42.112653
3504.644807	347566.434661	42.117658
3504.654121	347566.382305	42.122663
3504.782318	347548.698208	42.127668
3504.667080	347550.930793	42.132672
3504.852912	347538.506194	42.137677
3504.971370	347534.949625	42.142682
3504.502157	347528.075365	42.147687
3504.901694	347500.472882	42.152692
3504.928681	347508.282480	42.157696
3504.742400	347495.967606	42.162701
3504.862716	347478.259281	42.167706
3504.862161	347476.783159	42.172711
3505.166176	347459.758449	42.177716
3504.880730	347462.908776	42.182720
3504.547950	347437.636389	42.187725
3504.970282	347440.369392	42.192730
3504.659706	347429.321317	42.197735
3505.064553	347418.236489	42.202740
3504.721453	347409.229735	42.207744
3504.906966	347402.328306	42.212749
3504.730137	347396.476801	42.217754
3504.512779	347378.974545	42.222759
3504.830402	347368.412544	42.227764
3504.828860	347367.801953	42.232768
3504.717344	347358.096818	42.237773
3504.633485	347340.497087	42.242778
3504.614750	347349.561099	42.247783
3504.664053	347347.491687	42.252788
3504.481620	347329.347585	42.257792
3504.811148	347324.052327	42.262797
3504.666228	347328.427609	42.267802
3504.509376	347321.911178	42.272807
3504.604677	347299.905307	42.277812
3504.381429	347302.664024	42.282816
3504.509293	347299.971334	42.287821
3504.629023	347292.596696	42.292826
3504.244846	347291.664813	42.297831
3504.406003	347276.317037	42.302836
3504.423930	347268.882135	42.307840
3504.367206	347264.335151	42.312845
3504.767246	347270.609565	42.317850
3504.256618	347284.918184	42.322855
3504.950494	347271.751445	42.327860
3504.450407	347266.307366	42.332864
3504.571289	347255.929163	42.337869
3504.831390	347243.085519	42.342874
3504.635186	347237.618847	42.347879
3504.854487	347223.610840	42.352884
3504.828235	347235.246750	42.357888
3504.627371	347220.465241	42.362893
3504.814518	347200.379192	42.367898
3504.359989	347203.378098	42.372903
3504.637769	347195.240342	42.377908
3504.738333	347196.751608	42.382912
3504.702954	347183.165641	42.387917
3504.880447	347169.520565	42.392922
3504.868906	347172.093104	42.397927
3504.517464	347159.982436	42.402932
3504.672707	347153.594810	42.407936
3504.839038	347145.525571	42.412941
3504.785611	347130.313491	42.417946
3504.571958	347133.019795	42.422951
3504.717154	347114.772922	42.427956
3505.046563	347117.215203	42.432960
3504.254884	347099.472778	42.437965
3504.464349	347091.549426	42.442970
3504.489624	347089.356541	42.447975
3504.607767	347083.127488	42.452980
3504.682966	347087.798870	42.457984
3504.748448	347068.775560	42.462989
3504.897717	347055.694872	42.467994
3504.438859	347059.585307	42.472999
3504.649357	347048.836563	42.478004
3504.643521	347033.947815	42.483008
3504.596719	347035.151502	42.488013
3504.643646	347030.384492	42.493018
3504.353740	347022.031032	42.498023
3504.554639	347006.931425	42.503028
3504.265211	347004.151979	42.508032
3504.574664	347004.077623	42.513037
3504.647693	347010.149241	42.518042
3504.309184	347001.116245	42.523047
3504.494465	346993.934825	42.528052
3504.354345	346977.183809	42.533056
3504.495540	346982.633793	42.538061
3504.420048	346986.998125	42.543066
3504.452944	346991.523488	42.548071
3504.653181	346971.129859	42.553076
3504.349640	346960.131485	42.558080
3504.504232	346959.139870	42.563085
3504.793970	346955.556187	42.568090
3504.572316	346971.015465	42.573095
3504.447738	346945.200893	42.578100
3504.581439	346942.481811	42.583104
3504.341981	346947.126593	42.588109
3504.690501	346943.915403	42.593114
3504.563034	346947.040782	42.598119
3504.549502	346926.808197	42.603124
3504.589529	346921.787744	42.608128
3504.569367	346927.975914	42.613133
3504.871942	346926.986356	42.618138
3504.604869	346908.600976	42.623143
3504.458693	346889.687427	42.628148
3504.410674	346886.437116	42.633152
3504.538574	346898.175985	42.638157
3504.488102	346893.602531	42.643162
3504.375734	346882.039414	42.648167
3504.504053	346866.060407	42.653172
3504.253768	346856.249863	42.658176
3504.139357	346861.638459	42.663181
3504.508531	346865.550711	42.668186
3504.385155	346868.777258	42.673191
3504.587004	346850.979491	42.678196
3504.177743	346833.889195	42.683200
3503.977033	346835.880794	42.688205
3504.219457	346832.813634	42.693210
3504.361017	346843.379538	42.698215
3504.504071	346827.118212	42.703220
3504.247446	346840.139609	42.708224
3504.263033	346844.438647	42.713229
3504.412469	346833.623160	42.718234
3504.450280	346821.883573	42.723239
3504.283687	346804.933071	42.728244
3504.145864	346819.971895	42.733248
3504.186357	346817.394806	42.738253
3504.140752	346821.194469	42.743258
3504.080508	346823.240219	42.748263
3504.359600	346820.039999	42.753268
3504.249720	346831.791022	42.758272
3504.141475	346827.837558	42.763277
3504.509360	346795.912803	42.768282
3504.498831	346803.881144	42.773287
3504.621495	346802.767312	42.778292
3504.912732	346806.361006	42.783296
3504.487312	346788.560579	42.788301
3504.656530	346786.192210	42.793306
3504.359148	346789.166293	42.798311
3504.618328	346784.645685	42.803316
3504.415273	346766.886453	42.808321
3504.207798	346768.420979	42.813325
3504.536198	346764.831171	42.818330
3504.426080	346757.416445	42.823335
3504.295927	346757.055254	42.828340
3504.504992	346759.185693	42.833345
3504.506524	346758.956399	42.838349
3504.472091	346743.308518	42.843354
3504.348056	346740.604721	42.848359
3504.399664	346744.490831	42.853364
3504.011921	346730.069624	42.858369
3504.128973	346739.977654	42.863373
3504.168162	346726.150717	42.868378
3504.094758	346758.843478	42.873383
3504.340345	346742.794991	42.878388
3504.417169	346753.192977	42.883393
3504.475223	346720.859018	42.888397
3504.414590	346716.567135	42.893402
3503.972367	346722.338455	42.898407
3504.333084	346717.649073	42.903412
3504.748738	346706.562399	42.908417
3504.447134	346724.121498	42.913421
3504.653512	346717.725740	42.918426
3504.371408	346713.927017	42.923431
3504.387891	346703.641577	42.928436
3504.481601	346705.459371	42.933441
3504.582968	346696.305877	42.938445
3504.435380	346689.609740	42.943450
3504.233270	346672.308477	42.948455
3504.590203	346679.022466	42.953460
3504.721733	346680.223419	42.958465
3504.675327	346669.489768	42.963469
3504.814543	346655.265210	42.968474
3504.572508	346649.958443	42.973479
3504.840013	346634.084629	42.978484
3504.740408	346640.972611	42.983489
3504.501664	346618.713858	42.988493
3504.794371	346611.260880	42.993498
3504.315521	346618.361539	42.998503
3504.461024	346623.581803	43.003508
3504.702128	346601.730780	43.008513
3504.326220	346575.675797	43.013517
3504.514082	346577.809595	43.018522
3504.445960	346581.714644	43.023527
3504.544050	346585.084362	43.028532
3504.320204	346573.004302	43.033537
3504.137591	346589.144734	43.038541
3504.485143	346561.575470	43.043546
3504.209225	346557.852116	43.048551
3504.693727	346573.454387	43.053556
3504.631728	346566.821062	43.058561
3504.599781	346554.965186	43.063565
3504.543232	346531.888562	43.068570
3504.483205	346543.682668	43.073575
3504.617435	346533.862182	43.078580
3504.799897	346535.360518	43.083585
3504.913387	346504.061233	43.088589
3504.859048	346498.419345	43.093594
3504.689184	346510.358086	43.098599
3504.414006	346495.435423	43.103604
3504.479656	346471.117725	43.108609
3504.370194	346462.710201	43.113613
3504.823051	346468.314583	43.118618
3504.409083	346451.428539	43.123623
3504.579532	346444.045774	43.128628
3504.621089	346434.189018	43.133633
3504.431696	346434.778942	43.138637
3505.093747	346433.299846	43.143642
3504.728934	346421.292946	43.148647
3504.433685	346401.511958	43.153652
3504.542117	346409.996054	43.158657
3504.471958	346415.097715	43.163661
3504.416173	346392.122725	43.168666
3504.497753	346382.717782	43.173671
3504.470185	346372.413794	43.178676
3504.469914	346385.623840	43.183681
3504.336318	346377.881891	43.188685
3504.413743	346380.440400	43.193690
3504.216697	346369.323265	43.198695
3504.465811	346363.047975	43.203700
3504.577945	346350.176620	43.208705
3504.434074	346342.258122	43.213709
3504.465675	346353.783252	43.218714
3504.494477	346353.804173	43.223719
3504.445830	346337.649374	43.228724
3504.114726	346335.665520	43.233729
3504.366819	346338.730924	43.238733
3504.591882	346315.991483	43.243738
3504.244926	346331.725271	43.248743
3504.448621	346321.206542	43.253748
3504.371003	346308.008839	43.258753
3503.941564	346307.007736	43.263757
3503.901204	346309.788492	43.268762
3503.870530	346321.196211	43.273767
3504.169439	346303.713816	43.278772
3504.277174	346309.474587	43.283777
3504.376142	346308.364492	43.288781
3504.661596	346303.712428	43.293786
3504.143420	346313.084640	43.298791
3504.184098	346310.227518	43.303796
3504.100711	346318.996481	43.308801
3504.072360	346331.294678	43.313805
3504.302858	346321.102598	43.318810
3504.232547	346306.911080	43.323815
3504.043417	346293.247400	43.328820
3504.264172	346292.779822	43.333825
3504.412388	346297.668800	43.338829
3504.473546	346295.902909	43.343834
3504.037304	346324.733551	43.348839
3504.318107	346299.414559	43.353844
3504.615080	346293.055336	43.358849
3504.056769	346298.997768	43.363853
3504.520579	346258.403600	43.368858
3504.064679	346294.975018	43.373863
3504.276158	346261.954773	43.378868
3504.522410	346270.722533	43.383873
3504.182602	346284.444433	43.388877
3504.723359	346280.311966	43.393882
3504.404591	346253.967822	43.398887
3504.376480	346252.674194	43.403892
3504.212925	346258.834201	43.408897
3504.051896	346250.460252	43.413901
3504.139569	346242.530586	43.418906
3504.203808	346244.913016	43.423911
3504.192038	346266.727958	43.428916
3504.178580	346255.199984	43.433921
3503.922280	346267.101536	43.438925
3504.431151	346264.043126	43.443930
3504.299990	346262.689432	43.448935
3504.226411	346252.189075	43.453940
3504.009730	346243.111245	43.458945
3504.347197	346223.891937	43.463949
3504.420713	346224.185770	43.468954
3504.090518	346232.790143	43.473959
3504.414780	346238.618501	43.478964
3504.504657	346231.757503	43.483969
3504.385300	346235.823393	43.488973
3504.707404	346214.061230	43.493978
3504.356729	346216.534711	43.498983
3504.468796	346206.284976	43.503988
3504.796098	346217.585214	43.508993
3504.379039	346207.902737	43.513997
3504.657155	346184.136743	43.519002
3504.186146	346192.585215	43.524007
3504.753193	346171.293367	43.529012
3504.806157	346176.273773	43.534017
3504.255362	346177.124459	43.539021
3504.513199	346159.521249	43.544026
3504.293275	346152.836486	43.549031
3504.487861	346144.151771	43.554036
3504.546322	346147.731403	43.559041
3504.356904	346152.139262	43.564045
3504.642280	346134.378974	43.569050
3504.292304	346129.496469	43.574055
3504.448986	346131.635213	43.579060
3504.481060	346129.848463	43.584065
3504.120556	346130.210913	43.589069
3504.416571	346125.302637	43.594074
3504.186140	346123.201048	43.599079
3504.258315	346100.332976	43.604084
3503.697091	346101.872540	43.609089
3504.248172	346100.360074	43.614093
3504.600647	346089.894140	43.619098
3504.324630	346103.326016	43.624103
3504.453287	346101.320372	43.629108
3504.598984	346102.468191	43.634113
3504.245240	346108.963717	43.639117
3504.430695	346083.252459	43.644122
3504.379880	346077.940860	43.649127
3504.459942	346076.502861	43.654132
3504.211135	346074.531440	43.659137
3504.240152	346072.337925	43.664141
3504.509295	346072.244489	43.669146
3504.075457	346089.875593	43.674151
3504.064380	346080.408891	43.679156
3504.136260	346064.285867	43.684161
3504.114319	346055.533559	43.689165
3504.171375	346050.535791	43.694170
3504.179545	346057.254087	43.699175
3504.124277	346061.208045	43.704180
3504.003229	346052.089612	43.709185
3503.965543	346062.785810	43.714189
3504.298322	346058.228056	43.719194
3504.030347	346070.182399	43.724199
3504.574405	346057.268145	43.729204
3504.581845	346061.314001	43.734209
3504.357932	346054.375328	43.739213
3504.375636	346045.387675	43.744218
3504.336733	346051.629809	43.749223
3504.281089	346042.297411	43.754228
3504.278699	346041.712393	43.759233
3504.163718	346040.407041	43.764237
3504.511337	346039.817593	43.769242
3504.551140	346048.363498	43.774247
3504.298649	346020.481595	43.779252
3504.326481	346021.342615	43.784257
3504.360560	346005.810968	43.789261
3504.295045	346012.693636	43.794266
3504.189381	346020.575314	43.799271
3504.461700	346010.631096	43.804276
3504.466637	346013.430158	43.809281
3504.235800	346005.016304	43.814285
3504.399204	345984.373620	43.819290
3504.377009	345993.642017	43.824295
3504.421970	345991.853225	43.829300
3504.614402	345982.023445	43.834305
3504.250425	345984.499038	43.839309
3504.264532	345996.077912	43.844314
3504.072343	345972.564356	43.849319
3504.176265	345976.544058	43.854324
3504.638298	345970.133251	43.859329
3504.118176	345964.819480	43.864333
3504.263138	345963.931183	43.869338
3504.561503	345973.097997	43.874343
3504.558592	345968.262420	43.879348
3504.753538	345943.287735	43.884353
3504.472810	345922.918869	43.889357
3504.491201	345935.566102	43.894362
3503.981794	345944.249757	43.899367
3504.049217	345940.548441	43.904372
3504.032425	345935.333261	43.909377
3504.133872	345948.730949	43.914381
3504.208513	345949.839099	43.919386
3504.154543	345951.196659	43.924391
3504.232172	345935.810825	43.929396
3504.187157	345923.600544	43.934401
3504.264699	345925.980884	43.939405
3504.096641	345919.440612	43.944410
3504.330690	345920.243578	43.949415
3504.443132	345925.800020	43.954420
3505.011911	345921.408568	43.959425
3504.334124	345906.829386	43.964429
3504.691609	345898.220693	43.969434
3504.640869	345891.534604	43.974439
3504.255689	345899.053242	43.979444
3504.486245	345900.111291	43.984449
3504.084746	345886.379277	43.989453
3504.331459	345863.585329	43.994458
3503.957133	345862.219164	43.999463
3504.112359	345853.337004	44.004468
3503.950306	345868.558078	44.009473
3503.497629	345883.876002	44.014477
3504.235888	345864.542305	44.019482
3504.590117	345860.235674	44.024487
3504.437711	345867.768421	44.029492
3504.484133	345871.324521	44.034497
3504.342033	345872.059691	44.039501
3504.664776	345866.332672	44.044506
3504.477011	345852.490501	44.049511
3504.247800	345837.204058	44.054516
3504.678943	345832.248940	44.059521
3504.371029	345843.624225	44.064525
3504.554046	345839.242850	44.069530
3504.542341	345843.953525	44.074535
3504.741410	345816.509194	44.079540
3504.404083	345815.137177	44.084545
3504.584788	345818.035725	44.089549
3504.742002	345800.473768	44.094554
3504.498458	345792.418234	44.099559
3504.460867	345779.035910	44.104564
3504.596080	345768.986063	44.109569
3504.199847	345785.695005	44.114573
3504.542441	345770.674485	44.119578
3504.452872	345756.689501	44.124583
3504.264338	345748.421640	44.129588
3504.534668	345754.716728	44.134593
3504.330260	345750.345691	44.139597
3504.511697	345748.357144	44.144602
3504.310723	345755.159446	44.149607
3504.024803	345730.693395	44.154612
3504.146329	345725.634500	44.159617
3503.954481	345723.017735	44.164621
3504.194730	345711.907697	44.169626
3503.942605	345721.263395	44.174631
3504.133343	345718.407972	44.179636
3504.035574	345721.885065	44.184641
3504.093628	345724.192135	44.189645
3504.538761	345725.750776	44.194650
3504.325431	345739.936416	44.199655
3504.296777	345728.130756	44.204660
3504.436068	345739.613530	44.209665
3504.394896	345722.210179	44.214669
3504.667216	345704.706354	44.219674
3504.472889	345709.624084	44.224679
3504.272501	345701.052654	44.229684
3504.320847	345692.874600	44.234689
3504.142742	345699.036967	44.239693
3504.352054	345693.862378	44.244698
3503.787317	345691.279112	44.249703
3504.003724	345672.206027	44.254708
3503.796057	345675.293249	44.259713
3504.007916	345706.567039	44.264717
3504.272406	345703.445425	44.269722
3504.142953	345683.128918	44.274727
3504.251963	345672.472324	44.279732
3504.262027	345676.950493	44.284737
3504.146327	345686.182816	44.289741
3504.443551	345676.921837	44.294746
3503.686060	345702.494677	44.299751
3504.026063	345681.951231	44.304756
3504.332535	345687.018865	44.309761
3504.047928	345702.132093	44.314765
3504.112146	345700.136623	44.319770
3504.271613	345696.166209	44.324775
3504.210382	345704.117264	44.329780
3504.284516	345696.546007	44.334785
3503.939160	345697.262408	44.339789
3504.451839	345686.541996	44.344794
3504.642879	345666.225720	44.349799
3504.271818	345666.208046	44.354804
3504.371508	345669.043050	44.359809
3504.415464	345675.704826	44.364813
3504.409379	345673.160502	44.369818
3504.192019	345651.254339	44.374823
3504.279952	345639.150245	44.379828
3504.533815	345628.827084	44.384833
3503.976352	345644.823417	44.389837
3504.262436	345635.436927	44.394842
3504.082563	345639.868769	44.399847
3504.332379	345647.643391	44.404852
3504.410225	345642.005974	44.409857
3504.083449	345654.249683	44.414861
3504.388921	345642.569352	44.419866
3504.172563	345632.371439	44.424871
3504.058446	345616.532227	44.429876
3504.310851	345607.787385	44.434881
3503.998423	345625.373982	44.439885
3504.423418	345612.096657	44.444890
3504.286281	345621.688722	44.449895
3504.347321	345617.581145	44.454900
3504.470147	345626.928485	44.459905
3504.490299	345627.459835	44.464909
3504.413792	345594.942896	44.469914
3504.074142	345597.720097	44.474919
3504.142633	345588.622532	44.479924
3504.444609	345589.796560	44.484929
3504.024395	345599.382477	44.489933
3504.556777	345596.600301	44.494938
3504.475092	345597.122298	44.499943
3504.092948	345586.186995	44.504948
3504.463516	345577.907076	44.509953
3504.420792	345578.601085	44.514957
3504.759859	345561.366649	44.519962
3504.361573	345574.258008	44.524967
3504.494064	345565.812102	44.529972
3504.182505	345555.629227	44.534977
3503.876960	345543.892759	44.539981
3504.121677	345528.531307	44.544986
3504.252695	345543.731585	44.549991
3504.268048	345535.787804	44.554996
3504.262781	345537.672189	44.560001
3504.172605	345537.202857	44.565005
3504.367596	345547.429660	44.570010
3504.432171	345546.783144	44.575015
3503.927601	345546.252062	44.580020
3504.409184	345540.448993	44.585025
3504.202467	345535.798320	44.590029
3504.228432	345525.002109	44.595034
3504.067419	345521.642319	44.600039
3504.249272	345514.613977	44.605044
3504.056555	345517.724296	44.610049
3504.069210	345525.205538	44.615053
3503.947935	345520.210465	44.620058
3504.119705	345521.532346	44.625063
3504.160902	345527.965496	44.630068
3504.362950	345517.421430	44.635073
3503.859148	345543.437841	44.640077
3504.510718	345532.008208	44.645082
3504.373661	345534.549758	44.650087
3504.131264	345526.646725	44.655092
3504.044904	345505.279764	44.660097
3503.700602	345515.108225	44.665101
3504.348787	345524.550694	44.670106
3504.220818	345528.439823	44.675111
3504.172654	345509.663045	44.680116
3504.419613	345499.722750	44.685121
3504.298819	345509.744953	44.690125
3504.296030	345514.174261	44.695130
3504.366287	345509.327079	44.700135
3504.444138	345503.053319	44.705140
3504.576831	345494.301933	44.710145
3504.319500	345488.870211	44.715149
3504.391106	345483.870094	44.720154
3504.237744	345480.254561	44.725159
3504.415759	345477.782935	44.730164
3504.455642	345484.318111	44.735169
3504.217803	345485.882923	44.740173
3504.079785	345458.389903	44.745178
3504.072080	345449.482535	44.750183
3504.187085	345444.857351	44.755188
3504.321998	345444.708776	44.760193
3504.103546	345454.059193	44.765197
3504.502837	345450.127206	44.770202
3504.420890	345459.863291	44.775207
3504.279777	345462.252766	44.780212
3504.452900	345455.225797	44.785217
3504.502986	345443.153099	44.790221
3504.717869	345420.720355	44.795226
3504.281773	345432.955940	44.800231
3504.368791	345418.459347	44.805236
3504.421273	345418.501977	44.810241
3504.443897	345424.734450	44.815245
3504.391933	345404.787392	44.820250
3503.951575	345393.250380	44.825255
3503.910310	345387.326331	44.830260
3504.165699	345384.766110	44.835265
3504.249919	345383.327437	44.840269
3504.248095	345382.513244	44.845274
3504.409831	345394.628868	44.850279
3504.623614	345397.165862	44.855284
3504.577724	345401.398368	44.860289
3504.485506	345380.719524	44.865293
3504.236447	345352.047709	44.870298
3503.712541	345373.256718	44.875303
3504.048291	345371.752825	44.880308
3503.958263	345369.170853	44.885313
3504.062655	345374.957699	44.890317
3504.047648	345361.368084	44.895322
3503.880843	345373.713826	44.900327
3504.246836	345372.994201	44.905332
3504.390471	345371.597041	44.910337
3504.054356	345382.875061	44.915341
3504.217855	345372.795220	44.920346
3504.135169	345381.131510	44.925351
3504.415636	345383.403430	44.930356
3504.632320	345367.690024	44.935361
3503.956047	345331.297060	44.940365
3504.015991	345356.562644	44.945370
3503.984803	345353.004147	44.950375
3504.044597	345343.857012	44.955380
3504.492581	345339.204629	44.960385
3504.156557	345359.162185	44.965389
3504.293305	345360.642326	44.970394
3504.232480	345350.343415	44.975399
3504.301305	345348.296298	44.980404
3504.665681	345353.176634	44.985409
3504.334344	345341.469656	44.990413
3504.504862	345316.345845	44.995418
3504.296117	345311.619116	45.000423
3504.224900	345318.324594	45.005428
3504.413063	345322.520102	45.010433
3504.025154	345337.955194	45.015437
3504.333906	345318.154704	45.020442
3504.740101	345311.319949	45.025447
3504.332594	345293.465322	45.030452
3504.537299	345290.862203	45.035457
3504.483627	345292.397904	45.040461
3504.337840	345294.940844	45.045466
3504.250387	345285.307915	45.050471
3504.146600	345273.972200	45.055476
3504.190265	345259.660594	45.060481
3504.178094	345264.447750	45.065485
3504.001776	345259.715889	45.070490
3504.253763	345266.090290	45.075495
3504.123544	345263.311041	45.080500
3504.382188	345261.488444	45.085505
3504.436411	345267.079607	45.090509
3504.456148	345260.051411	45.095514
3504.476920	345264.680639	45.100519
3504.549898	345238.706806	45.105524
3504.242211	345226.436094	45.110529
3503.949640	345231.573022	45.115533
3504.319568	345224.260379	45.120538
3504.248906	345227.605949	45.125543
3503.878887	345241.129244	45.130548
3504.055558	345233.134463	45.135553
3504.030092	345239.170933	45.140557
3504.310131	345235.792304	45.145562
3504.283934	345246.715913	45.150567
3504.341221	345231.918535	45.155572
3504.374040	345220.815745	45.160577
3503.991475	345220.596263	45.165581
3504.326865	345208.300238	45.170586
3504.114097	345210.930131	45.175591
3504.238776	345206.761557	45.180596
3504.689392	345213.868158	45.185601
3504.035645	345208.219097	45.190605
3504.267396	345209.353329	45.195610
3503.967110	345214.211493	45.200615
3503.971838	345211.029108	45.205620
3504.215221	345213.434164	45.210625
3504.140148	345200.159447	45.215629
3504.398264	345195.358898	45.220634
3504.428254	345194.208780	45.225639
3504.388210	345187.062761	45.230644
3504.544804	345187.445277	45.235649
3504.107284	345184.205543	45.240653
3504.319417	345179.794062	45.245658
3504.165093	345185.825456	45.250663
3504.257549	345171.277035	45.255668
3504.220945	345162.068752	45.260673
3504.046876	345166.525166	45.265677
3504.393391	345156.899966	45.270682
3504.319708	345169.231029	45.275687
3504.176054	345176.100696	45.280692
3504.323418	345171.572187	45.285697
3504.208051	345173.372178	45.290701
3503.947630	345172.624319	45.295706
3504.039576	345172.075285	45.300711
3503.904322	345171.256731	45.305716
3504.432869	345164.835321	45.310721
3504.180000	345175.947500	45.315725
3504.130060	345156.712730	45.320730
3504.068872	345158.300529	45.325735
3504.004088	345140.773471	45.330740
3504.022791	345139.090618	45.335745
3503.983472	345147.852790	45.340749
3503.932486	345157.914923	45.345754
3504.047198	345144.915628	45.350759
3503.731448	345147.383632	45.355764
3504.041623	345153.137966	45.360769
3503.897979	345153.695217	45.365773
3503.653587	345150.704934	45.370778
3504.078598	345184.007022	45.375783
3503.973818	345184.252689	45.380788
3504.089695	345188.383274	45.385793
3503.829312	345186.948172	45.390797
3504.077734	345184.236323	45.395802
3504.226231	345189.328976	45.400807
3504.013447	345179.384952	45.405812
3504.237811	345158.961418	45.410817
3504.206747	345169.071306	45.415821
3504.420508	345172.270100	45.420826
3504.163500	345175.797853	45.425831
3503.998126	345170.860629	45.430836
3504.449728	345174.581792	45.435841
3504.099887	345179.575060	45.440845
3504.195206	345174.545714	45.445850
3504.479906	345175.442496	45.450855
3504.213583	345181.746130	45.455860
3504.600125	345149.893882	45.460865
3504.247084	345148.397067	45.465869
3504.041539	345147.640532	45.470874
3504.029426	345161.158168	45.475879
3504.237394	345147.940503	45.480884
3504.350795	345141.966524	45.485889
3504.368938	345149.319680	45.490893
3504.237896	345145.267891	45.495898
3504.434954	345142.284175	45.500903
3504.036186	345133.234959	45.505908
3504.579205	345118.742558	45.510913
3504.311997	345123.239153	45.515917
3504.221647	345109.177778	45.520922
3504.200629	345136.187081	45.525927
3504.341234	345120.485637	45.530932
3504.444170	345117.771333	45.535937
3504.138518	345119.423236	45.540941
3504.581107	345086.416693	45.545946
3504.164749	345091.420484	45.550951
3504.134774	345092.952444	45.555956
3504.213897	345085.380319	45.560961
3503.868867	345099.459668	45.565965
3503.863540	345085.690285	45.570970
3503.886948	345098.922333	45.575975
3504.147717	345087.579852	45.580980
3504.207950	345092.253762	45.585985
3504.182354	345097.857560	45.590989
3504.439176	345089.977355	45.595994
3504.086619	345088.378649	45.600999
3504.171861	345100.506427	45.606004
3504.328090	345095.772885	45.611009
3504.027939	345097.907531	45.616013
3504.013635	345078.845275	45.621018
3503.951478	345073.713551	45.626023
3504.090426	345069.339085	45.631028
3504.127148	345071.216847	45.636033
3503.896352	345071.558797	45.641037
3504.329344	345070.726763	45.646042
3504.303950	345070.985332	45.651047
3504.126611	345069.689817	45.656052
3504.504605	345072.200864	45.661057
3504.148323	345075.617052	45.666061
3504.416797	345075.905521	45.671066
3504.157533	345088.520474	45.676071
3504.099285	345080.613720	45.681076
3504.467974	345057.545641	45.686081
3504.068171	345058.881537	45.691085
3504.482935	345053.547144	45.696090
3504.411177	345054.143937	45.701095
3503.988168	345061.668663	45.706100
3504.129197	345047.214345	45.711105
3504.306712	345066.912637	45.716109
3504.533506	345058.553562	45.721114
3504.099177	345055.516943	45.726119
3504.168399	345041.532136	45.731124
3504.487898	345016.155563	45.736129
3504.096492	345024.922512	45.741133
3504.376731	345004.235557	45.746138
3504.647156	345016.054088	45.751143
3504.452492	345034.080404	45.756148
3504.705949	345014.924888	45.761153
3504.321240	344997.168380	45.766157
3504.726448	344986.159391	45.771162
3504.164084	344984.390226	45.776167
3504.297370	344991.114317	45.781172
3504.182844	344989.121628	45.786177
3503.943533	344989.770365	45.791181
3504.416610	344987.404790	45.796186
3504.414864	344977.656447	45.801191
3504.314207	344955.909746	45.806196
3504.162270	344948.246867	45.811201
3504.120372	344959.656627	45.816205
3504.509244	344944.424952	45.821210
3504.413105	344952.992510	45.826215
3504.280984	344948.686344	45.831220
3504.578541	344951.515554	45.836225
3504.297533	344935.982530	45.841229
3504.264327	344923.515639	45.846234
3504.012985	344922.868156	45.851239
3504.127392	344925.446335	45.856244
3504.210285	344920.978907	45.861249
3503.863744	344934.829455	45.866253
3503.983959	344931.756063	45.871258
3503.863004	344931.317046	45.876263
3503.973838	344928.601485	45.881268
3504.235174	344919.549688	45.886273
3503.850995	344936.893300	45.891277
3504.302404	344934.607509	45.896282
3504.169959	344936.461114	45.901287
3504.010804	344931.548340	45.906292
3504.325325	344936.385686	45.911297
3504.370941	344936.123962	45.916301
3504.294878	344919.311316	45.921306
3504.227736	344913.544031	45.926311
3503.842150	344907.827091	45.931316
3503.743342	344905.322847	45.936321
3504.030712	344902.172120	45.941325
3504.370655	344910.059858	45.946330
3504.301615	344904.649220	45.951335
3504.130201	344910.123369	45.956340
3504.381916	344904.942007	45.961345
3504.098288	344915.422763	45.966349
3504.500408	344910.981225	45.971354
3504.111590	344910.788184	45.976359
3504.158175	344919.765890	45.981364
3504.507810	344903.522272	45.986369
3504.358665	344901.076893	45.991373
3504.424557	344882.689136	45.996378
3504.375862	344881.093291	46.001383
3504.426049	344863.827961	46.006388
3504.173609	344873.031123	46.011393
3504.042687	344885.804003	46.016397
3504.540131	344872.973219	46.021402
3504.414523	344864.466203	46.026407
3504.150560	344853.970240	46.031412
3504.340450	344843.580695	46.036417
3504.153178	344855.446167	46.041421
3504.274280	344851.659935	46.046426
3504.168340	344856.181961	46.051431
3504.285637	344851.861809	46.056436
3504.505308	344846.736415	46.061441
3504.481137	344843.253138	46.066445
3504.500288	344821.996515	46.071450
3504.391523	344821.351942	46.076455
3503.883691	344821.355891	46.081460
3504.327358	344815.686012	46.086465
3504.051803	344812.675185	46.091469
3504.029009	344812.144287	46.096474
3504.031074	344814.256618	46.101479
3504.008593	344826.477844	46.106484
3504.387486	344821.327275	46.111489
3503.774391	344829.034803	46.116493
3504.247062	344817.836943	46.121498
3504.041772	344826.141788	46.126503
3504.076441	344824.201867	46.131508
3504.427497	344819.030245	46.136513
3504.464062	344802.250667	46.141517
3504.390312	344790.121052	46.146522
3504.445813	344786.217921	46.151527
3504.349850	344790.738374	46.156532
3504.713982	344794.727925	46.161537
3504.393108	344775.357691	46.166541
3504.472092	344766.105619	46.171546
3504.373635	344768.106576	46.176551
3504.145380	344774.047887	46.181556
3504.543624	344764.770793	46.186561
3504.402326	344767.440313	46.191565
3504.125136	344755.571937	46.196570
3503.917267	344741.961762	46.201575
3503.864886	344732.094116	46.206580
3503.947548	344729.866616	46.211585
3504.063332	344757.439895	46.216589
3504.168145	344749.990933	46.221594
3504.237437	344745.347468	46.226599
3504.186597	344736.294090	46.231604
3504.343711	344735.887470	46.236609
3503.977004	344736.836338	46.241613
3504.015426	344735.506704	46.246618
3503.890935	344736.646360	46.251623
3504.194302	344743.267229	46.256628
3504.371942	344739.472052	46.261633
3504.012724	344754.266424	46.266637
3504.173268	344753.070204	46.271642
3503.975534	344753.076033	46.276647
3504.053085	344754.183746	46.281652
3504.108821	344747.404333	46.286657
3503.906665	344749.701673	46.291661
3504.144613	344754.042072	46.296666
3504.369970	344746.599505	46.301671
3503.783788	344753.208289	46.306676
3504.327812	344749.787896	46.311681
3504.210972	344743.112126	46.316685
3504.071593	344725.240390	46.321690
3504.211438	344708.800805	46.326695
3504.215480	344718.625232	46.331700
3504.357876	344713.435683	46.336705
3504.336837	344708.984671	46.341709
3504.402406	344721.319265	46.346714
3504.357880	344725.373429	46.351719
3504.202818	344727.485151	46.356724
3504.356045	344711.552520	46.361729
3504.091280	344704.161982	46.366733
3503.991050	344690.585685	46.371738
3504.483006	344689.846138	46.376743
3504.323482	344680.453586	46.381748
3504.261315	344684.154192	46.386753
3504.401942	344687.313668	46.391757
3504.440988	344702.045088	46.396762
3504.294032	344690.614271	46.401767
3504.307041	344665.438724	46.406772
3504.511427	344653.239655	46.411777
3504.300124	344658.058343	46.416781
3503.906864	344663.338507	46.421786
3504.450804	344657.525493	46.426791
3504.053320	344660.388241	46.431796
3504.232446	344658.120034	46.436801
3504.398125	344667.409845	46.441805
3504.471121	344655.893340	46.446810
3504.055097	344636.461743	46.451815
3503.958391	344640.218720	46.456820
3504.360314	344625.366703	46.461825
3503.972766	344624.511668	46.466829
3504.250612	344620.675187	46.471834
3504.593609	344624.566277	46.476839
3504.423107	344622.989682	46.481844
3504.414908	344630.576149	46.486849
3504.360566	344623.050519	46.491853
3504.199415	344598.487909	46.496858
3504.205092	344595.127166	46.501863
3504.199460	344594.415379	46.506868
3504.239546	344590.565578	46.511873
3503.922224	344604.233409	46.516877
3503.977269	344589.054420	46.521882
3504.169271	344608.216051	46.526887
3503.900498	344608.156750	46.531892
3504.050566	344604.569552	46.536897
3503.380914	344612.947841	46.541901
3503.849719	344605.084965	46.546906
3504.020279	344603.199913	46.551911
3504.017841	344612.134508	46.556916
3504.260021	344598.096799	46.561921
3504.180255	344602.640160	46.566925
3504.058793	344593.521565	46.571930
3504.402817	344600.263290	46.576935
3504.252794	344604.817759	46.581940
3504.343832	344610.683152	46.586945
3504.311097	344614.506378	46.591949
3504.315017	344570.980231	46.596954
3504.209501	344576.749436	46.601959
3504.158975	344577.928308	46.606964
3504.182302	344571.128545	46.611969
3504.327048	344577.494521	46.616973
3504.264221	344560.781495	46.621978
3504.557572	344575.650916	46.626983
3504.586090	344566.024988	46.631988
3504.701175	344559.388892	46.636993
3504.238095	344556.458606	46.641997
3504.143739	344547.208451	46.647002
3504.243623	344538.411203	46.652007
3503.850540	344539.644234	46.657012
3504.215213	344542.182864	46.662017
3504.247718	344540.370543	46.667021
3504.549189	344539.788377	46.672026
3504.036825	344529.026185	46.677031
3504.013904	344529.946158	46.682036
3504.270214	344519.062438	46.687041
3504.040746	344517.393349	46.692045
3504.434362	344508.829647	46.697050
3504.247146	344512.422767	46.702055
3503.664285	344510.224116	46.707060
3504.194609	344508.663986	46.712065
3504.306811	344510.173483	46.717069
3504.448104	344500.987879	46.722074
3504.649511	344501.490583	46.727079
3504.151340	344513.939801	46.732084
3504.272959	344504.960937	46.737089
3504.197290	344491.329804	46.742093
3504.212640	344478.982410	46.747098
3504.364491	344482.140122	46.752103
3504.324563	344484.895443	46.757108
3504.390877	344485.394051	46.762113
3503.921270	344493.613463	46.767117
3504.136872	344482.685264	46.772122
3504.503093	344494.845105	46.777127
3504.365199	344486.059988	46.782132
3504.311287	344469.065537	46.787137
3504.317465	344460.537629	46.792141
3504.407615	344450.112876	46.797146
3504.002245	344456.107674	46.802151
3504.230653	344452.228091	46.807156
3504.441463	344451.711165	46.812161
3504.508984	344460.456548	46.817165
3504.342347	344447.985199	46.822170
3504.024577	344429.581597	46.827175
3503.833553	344430.757231	46.832180
3504.280288	344426.104974	46.837185
3503.795486	344429.006992	46.842189
3503.762257	344427.281422	46.847194
3503.950913	344434.505894	46.852199
3503.906508	344423.262442	46.857204
3503.964339	344421.497020	46.862209
3503.925077	344436.469970	46.867213
3504.236032	344442.300612	46.872218
3504.115522	344444.966860	46.877223
3504.099703	344438.275084	46.882228
3504.213179	344433.446434	46.887233
3503.982467	344441.220826	46.892237
3503.770752	344430.920156	46.897242
3504.185168	344432.407328	46.902247
3503.670512	344448.422671	46.907252
3504.310489	344431.878485	46.912257
3503.911332	344446.093816	46.917261
3504.119355	344432.163281	46.922266
3504.006841	344452.314890	46.927271
3504.157837	344446.691247	46.932276
3504.263223	344450.339925	46.937281
3504.158011	344448.091209	46.942285
3503.728479	344432.123370	46.947290
3504.086778	344449.986080	46.952295
3503.745668	344462.537746	46.957300
3504.037499	344443.808688	46.962305
3503.920958	344442.350826	46.967309
3504.059322	344462.793664	46.972314
3504.176031	344434.801728	46.977319
3504.129071	344457.030166	46.982324
3504.429925	344451.713728	46.987329
3504.135209	344454.432971	46.992333
3504.062429	344466.025884	46.997338
3504.608365	344452.780085	47.002343
3503.989012	344446.667348	47.007348
3504.778566	344410.703862	47.012353
3504.123204	344425.137879	47.017357
3504.104012	344408.443364	47.022362
3504.599232	344424.171785	47.027367
3504.531795	344432.709426	47.032372
3504.828768	344411.230557	47.037377
3504.344918	344383.715349	47.042381
3504.235690	344392.590500	47.047386
3504.422917	344384.975741	47.052391
3503.897409	344380.273563	47.057396
3504.586339	344376.473889	47.062401
3504.186931	344383.511350	47.067405
3504.159414	344375.650550	47.072410
3504.196183	344368.008669	47.077415
3504.179484	344353.833654	47.082420
3504.294010	344343.634112	47.087425
3504.032350	344354.213309	47.092429
3504.218556	344350.034948	47.097434
3504.002076	344355.770810	47.102439
3504.438783	344351.196494	47.107444
3504.301854	344349.767306	47.112449
3504.144576	344367.202480	47.117453
3504.376918	344349.806388	47.122458
3504.212645	344339.421840	47.127463
3504.222025	344336.747745	47.132468
3504.337283	344321.660983	47.137473
3504.263949	344339.133802	47.142477
3504.344273	344328.481499	47.147482
3503.940692	344327.985346	47.152487
3504.237920	344332.570940	47.157492
3503.975779	344333.172385	47.162497
3503.974713	344345.695769	47.167501
3504.148227	344329.887097	47.172506
3504.324726	344342.306047	47.177511
3503.997750	344335.332556	47.182516
3504.113840	344337.248701	47.187521
3504.105863	344348.907752	47.192525
3503.994127	344337.649474	47.197530
3503.914703	344333.487654	47.202535
3504.064958	344336.543811	47.207540
3504.511044	344327.208179	47.212545
3503.973710	344322.787855	47.217549
3504.397944	344298.692552	47.222554
3504.412694	344306.148164	47.227559
3503.968122	344303.520384	47.232564
3504.168167	344306.085052	47.237569
3504.222433	344305.312883	47.242573
3504.379714	344307.171609	47.247578
3504.377026	344308.928358	47.252583
3504.203201	344316.795587	47.257588
3503.939243	344300.623359	47.262593
3503.623211	344290.924591	47.267597
3503.892135	344300.605395	47.272602
3504.067581	344303.912108	47.277607
3504.116415	344319.558408	47.282612
3504.076329	344313.735880	47.287617
3504.344783	344302.086590	47.292621
3504.455288	344284.124306	47.297626
3504.123658	344279.162385	47.302631
3504.121906	344282.649836	47.307636
3504.188696	344269.199758	47.312641
3503.925750	344282.986334	47.317645
3503.825787	344279.082294	47.322650
3504.034169	344278.463936	47.327655
3503.697637	344285.338746	47.332660
3504.155597	344273.124963	47.337665
3503.820236	344286.413913	47.342669
3504.060645	344283.245124	47.347674
3503.847668	344287.453219	47.352679
3503.918778	344279.424091	47.357684
3504.156374	344274.219453	47.362689
3503.855415	344297.735338	47.367693
3504.035768	344288.568980	47.372698
3504.076824	344286.398948	47.377703
3503.917402	344293.856644	47.382708
3504.138666	344298.912417	47.387713
3504.082922	344292.252391	47.392717
3504.210797	344285.130622	47.397722
3504.139596	344299.370499	47.402727
3503.794047	344289.676397	47.407732
3504.076482	344290.853542	47.412737
3503.899737	344305.033743	47.417741
3503.907847	344296.098247	47.422746
3504.058931	344287.191052	47.427751
3503.932793	344293.345349	47.432756
3504.027633	344287.781477	47.437761
3504.291699	344295.375849	47.442765
3504.482789	344291.985775	47.447770
3504.487478	344299.570247	47.452775
3504.378119	344283.449933	47.457780
3504.565857	344259.315643	47.462785
3504.181709	344267.165223	47.467789
3504.034791	344262.606810	47.472794
3504.382215	344256.010308	47.477799
3504.336684	344265.995370	47.482804
3504.322011	344269.535772	47.487809
3504.412162	344273.594128	47.492813
3504.085488	344263.642501	47.497818
3503.833193	344246.806619	47.502823
3503.772030	344249.616216	47.507828
3504.189095	344252.757463	47.512833
3504.302548	344258.670255	47.517837
3504.280202	344241.085314	47.522842
3504.450544	344234.491352	47.527847
3504.388133	344242.340976	47.532852
3504.283341	344241.975760	47.537857
3504.281903	344248.135800	47.542861
3504.398826	344245.011986	47.547866
3504.208520	344223.686448	47.552871
3503.933991	344219.122753	47.557876
3504.141228	344205.752272	47.562881
3503.793626	344199.800174	47.567885
3503.674338	344198.724545	47.572890
3504.119309	344216.268179	47.577895
3503.776570	344223.729412	47.582900
3503.912191	344229.435073	47.587905
3504.017357	344243.494358	47.592909
3504.079827	344249.186128	47.597914
3504.458590	344238.562987	47.602919
3504.110577	344219.375037	47.607924
3504.287403	344213.034585	47.612929
3504.240169	344216.783768	47.617933
3504.314231	344209.950488	47.622938
3504.488725	344209.032042	47.627943
3504.136819	344217.156522	47.632948
3504.207021	344213.021945	47.637953
3504.342840	344214.018641	47.642957
3504.465072	344205.370533	47.647962
3504.052400	344182.120201	47.652967
3504.104163	344185.141030	47.657972
3504.402527	344179.188619	47.662977
3504.246293	344182.445962	47.667981
3504.245864	344179.518874	47.672986
3504.337596	344178.664420	47.677991
3504.082291	344173.944959	47.682996
3504.299819	344175.845072	47.688001
3504.160982	344183.604972	47.693005
3504.554237	344166.768821	47.698010
3504.371639	344156.438046	47.703015
3504.118674	344145.023884	47.708020
3504.459697	344145.606333	47.713025
3504.371525	344143.991255	47.718029
3504.344502	344146.719098	47.723034
3504.222664	344151.396413	47.728039
3504.175700	344147.178541	47.733044
3504.198657	344118.895834	47.738049
3503.736726	344116.118067	47.743053
3504.158519	344118.393147	47.748058
3504.147147	344118.191336	47.753063
3503.815285	344123.029127	47.758068
3504.145339	344120.075241	47.763073
3503.968073	344118.041535	47.768077
3504.086679	344116.775571	47.773082
3504.100126	344132.503876	47.778087
3504.274949	344119.749389	47.783092
3504.430652	344121.481102	47.788097
3504.364172	344126.047853	47.793101
3504.434336	344125.120446	47.798106
3504.312139	344121.525356	47.803111
3504.032776	344123.656751	47.808116
3504.108680	344097.656499	47.813121
3504.259335	344095.698217	47.818125
3504.054735	344097.919608	47.823130
3504.302171	344088.513529	47.828135
3504.214056	344098.148999	47.833140
3504.328314	344088.356716	47.838145
3504.134200	344089.176492	47.843149
3504.425009	344083.963425	47.848154
3504.679383	344069.083689	47.853159
3503.982877	344074.691839	47.858164
3504.233640	344055.205540	47.863169
3504.152931	344051.731155	47.868173
3504.092852	344049.118936	47.873178
3504.259425	344053.903384	47.878183
3504.222457	344066.661587	47.883188
3504.170118	344060.510072	47.888193
3503.911679	344069.357954	47.893197
3503.906213	344056.428327	47.898202
3504.418634	344061.209004	47.903207
3503.888670	344063.889096	47.908212
3504.128265	344055.655125	47.913217
3504.210295	344063.201945	47.918221
3504.472173	344072.222103	47.923226
3504.389810	344064.955370	47.928231
3503.792780	344043.286810	47.933236
3504.382966	344024.714081	47.938241
3504.296908	344018.007910	47.943245
3504.133606	344026.306228	47.948250
3504.366764	344020.898639	47.953255
3504.312378	344024.776233	47.958260
3504.173342	344022.761933	47.963265
3503.952138	344026.207733	47.968269
3503.981556	344028.443036	47.973274
3503.902888	344028.175503	47.978279
3504.003295	344025.512457	47.983284
3504.466270	344029.002811	47.988289
3504.117259	344029.592540	47.993293
3504.295070	344029.946256	47.998298
3504.578050	344014.552908	48.003303
3503.857489	344006.852537	48.008308
3504.100813	344000.527003	48.013313
3504.124335	344006.657668	48.018317
3504.430397	343993.449691	48.023322
3504.237349	343996.432873	48.028327
3504.259351	344001.087460	48.033332
3504.434372	343986.143887	48.038337
3503.872216	343993.512570	48.043341
3504.002582	344006.549775	48.048346
3504.105939	343993.119308	48.053351
3504.077169	343998.494628	48.058356
3504.031534	344001.709041	48.063361
3503.990539	343987.817773	48.068365
3503.940397	343976.447873	48.073370
3504.108269	343973.595982	48.078375
3504.028849	343971.317717	48.083380
3504.307346	343962.084885	48.088385
3504.089438	343967.464656	48.093389
3503.897417	343961.335214	48.098394
3504.307650	343966.641131	48.103399
3504.174323	343971.091193	48.108404
3504.345911	343969.536858	48.113409
3504.329986	343973.713821	48.118413
3504.477216	343964.349019	48.123418
3504.292304	343978.937849	48.128423
3504.091968	343972.809724	48.133428
3504.315277	343948.313331	48.138433
3504.407760	343951.989533	48.143437
3504.139757	343946.355725	48.148442
3504.072267	343943.006513	48.153447
3504.184662	343945.483238	48.158452
3504.473247	343929.783537	48.163457
3504.361628	343947.949776	48.168461
3504.438210	343937.297995	48.173466
3504.223987	343928.906670	48.178471
3503.799239	343911.359797	48.183476
3504.330663	343904.352359	48.188481
3504.189833	343904.425553	48.193485
3504.290336	343904.766038	48.198490
3504.356183	343905.341087	48.203495
3504.005214	343917.716249	48.208500
3504.435769	343910.495674	48.213505
3504.211062	343915.469264	48.218509
3504.375541	343915.239650	48.223514
3504.211622	343926.363454	48.228519
3504.251737	343898.536099	48.233524
3504.080270	343892.123409	48.238529
3504.027099	343891.011867	48.243533
3503.895147	343888.970989	48.248538
3504.134160	343892.954929	48.253543
3504.188137	343888.212002	48.258548
3504.411860	343878.835094	48.263553
3504.095090	343884.739579	48.268557
3504.151272	343898.068529	48.273562
3504.365609	343894.725665	48.278567
3503.901372	343893.551843	48.283572
3504.102705	343880.309492	48.288577
3504.259250	343887.691831	48.293581
3504.095024	343899.910203	48.298586
3504.238877	343890.622285	48.303591
3504.153195	343892.163083	48.308596
3504.094086	343869.187630	48.313601
3504.089450	343866.337553	48.318605
3504.164742	343862.049424	48.323610
3503.996926	343849.476320	48.328615
3503.972240	343860.629031	48.333620
3504.372693	343841.704435	48.338625
3504.255832	343865.293200	48.343629
3504.180772	343855.149002	48.348634
3504.242794	343853.331994	48.353639
3503.947328	343854.040528	48.358644
3504.243511	343848.241152	48.363649
3504.261435	343858.445334	48.368653
3504.097169	343861.907596	48.373658
3503.972309	343858.567449	48.378663
3503.739187	343871.254889	48.383668
3504.193779	343855.325291	48.388673
3503.979816	343874.882241	48.393677
3503.965358	343868.648356	48.398682
3503.951239	343871.348717	48.403687
3504.061695	343867.945914	48.408692
3504.109863	343873.894520	48.413697
3504.069169	343867.104798	48.418701
3503.993696	343861.364181	48.423706
3504.261461	343845.718657	48.428711
3503.946565	343847.524779	48.433716
3504.451905	343834.692523	48.438721
3503.985098	343834.893615	48.443725
3503.996725	343831.964604	48.448730
3504.301738	343838.610768	48.453735
3503.976992	343831.407781	48.458740
3504.337279	343833.030796	48.463745
3504.164183	343831.607313	48.468749
3504.203617	343828.113921	48.473754
3504.599733	343830.876695	48.478759
3504.134012	343835.099326	48.483764
3504.221427	343833.227395	48.488769
3504.061249	343819.787645	48.493773
3503.837626	343809.896012	48.498778
3504.028530	343804.265999	48.503783
3504.256203	343800.870114	48.508788
3504.265896	343788.905280	48.513793
3504.076386	343807.312962	48.518797
3503.960613	343807.840364	48.523802
3504.496757	343801.239429	48.528807
3504.143438	343797.019059	48.533812
3504.413102	343805.579856	48.538817
3504.160067	343811.906988	48.543821
3504.116461	343793.154398	48.548826
3504.395996	343805.022639	48.553831
3504.059093	343797.974293	48.558836
3504.095861	343773.329143	48.563841
3504.172201	343778.789680	48.568845
3504.011561	343769.829876	48.573850
3504.291164	343771.516557	48.578855
3503.941877	343771.266353	48.583860
3504.131299	343771.032796	48.588865
3504.033658	343768.019241	48.593869
3503.881696	343771.734101	48.598874
3504.301356	343769.682371	48.603879
3504.119945	343773.300071	48.608884
3504.267553	343759.582563	48.613889
3504.261080	343765.183464	48.618893
3504.110625	343769.763518	48.623898
3504.400218	343777.099382	48.628903
3503.791645	343780.479169	48.633908
3503.922298	343783.003922	48.638913
3504.144603	343786.481433	48.643917
3504.008388	343787.750230	48.648922
3504.290856	343786.356537	48.653927
3503.917707	343773.764972	48.658932
3504.141517	343744.101278	48.663937
3503.910353	343747.523214	48.668941
3504.070311	343754.141413	48.673946
3504.415657	343737.465439	48.678951
3504.072311	343741.439644	48.683956
3504.170924	343745.903961	48.688961
3504.147008	343748.962231	48.693965
3504.057595	343761.194257	48.698970
3503.850261	343744.885657	48.703975
3503.944101	343761.619505	48.708980
3504.352267	343748.013524	48.713985
3504.110495	343753.651626	48.718989
3503.956597	343755.890467	48.723994
3504.239382	343764.092841	48.728999
3503.958977	343753.319290	48.734004
3504.061625	343756.077557	48.739009
3504.233619	343760.835718	48.744013
3504.114926	343743.113138	48.749018
3504.202784	343751.906318	48.754023
3504.249755	343760.298698	48.759028
3504.372778	343737.854386	48.764033
3504.310631	343726.409975	48.769037
3504.408010	343728.965445	48.774042
3504.316134	343731.703560	48.779047
3504.285420	343731.835706	48.784052
3504.413962	343726.851894	48.789057
3504.156244	343739.645066	48.794061
3504.326975	343719.865864	48.799066
3504.315648	343700.700878	48.804071
3503.934355	343697.299448	48.809076
3504.277198	343679.376612	48.814081
3504.041117	343682.061166	48.819085
3504.230767	343692.187319	48.824090
3504.177803	343687.614008	48.829095
3503.986419	343685.557065	48.834100
3504.060266	343680.938250	48.839105
3504.184032	343688.860329	48.844109
3504.222850	343683.152534	48.849114
3504.408544	343673.450704	48.854119
3504.100507	343688.797235	48.859124
3504.176084	343686.596270	48.864129
3504.287851	343678.687904	48.869133
3504.316066	343674.559928	48.874138
3503.956619	343659.471688	48.879143
3503.938972	343664.998003	48.884148
3504.025313	343652.155590	48.889153
3504.314632	343663.055062	48.894157
3504.175914	343665.596954	48.899162
3504.424500	343658.226941	48.904167
3504.230470	343661.439380	48.909172
3504.515187	343649.711030	48.914177
3504.449054	343664.459336	48.919181
3504.133988	343652.036740	48.924186
3504.361229	343621.583370	48.929191
3504.229796	343626.313152	48.934196
3504.257984	343606.480086	48.939201
3504.093085	343624.756663	48.944205
3503.977371	343621.415057	48.949210
3504.203217	343620.157582	48.954215
3503.962209	343628.417332	48.959220
3504.065862	343627.764617	48.964225
3503.822122	343629.457680	48.969229
3504.038158	343630.467158	48.974234
3503.928731	343622.008314	48.979239
3504.142062	343624.596365	48.984244
3504.307704	343627.013777	48.989249
3504.046665	343636.651207	48.994253
3504.310171	343628.718844	48.999258
3504.332246	343625.075461	49.004263
3503.948895	343623.532490	49.009268
3504.015287	343602.497048	49.014273
3504.127555	343586.901494	49.019277
3504.304507	343598.633270	49.024282
3504.086618	343598.947733	49.029287
3503.937319	343592.327874	49.034292
3504.135132	343585.678590	49.039297
3503.808312	343604.922569	49.044301
3503.631051	343599.732553	49.049306
3504.135275	343594.256617	49.054311
3503.817947	343601.637548	49.059316
3503.778332	343597.622107	49.064321
3503.910011	343615.597258	49.069325
3503.871804	343624.563111	49.074330
3504.082626	343617.097247	49.079335
3504.079989	343633.260943	49.084340
3504.293094	343612.889566	49.089345
3503.868649	343616.927509	49.094349
3503.886853	343607.812135	49.099354
3504.293146	343610.267864	49.104359
3503.730609	343620.105686	49.109364
3503.918545	343615.825184	49.114369
3504.096150	343614.600791	49.119373
3503.942120	343601.923639	49.124378
3504.249932	343615.034691	49.129383
3503.977179	343615.968723	49.134388
3504.292464	343613.348048	49.139393
3504.361935	343614.100704	49.144397
3504.059549	343612.697657	49.149402
3504.511838	343610.335316	49.154407
3504.274413	343615.056401	49.159412
3504.269247	343611.748225	49.164417
3504.396440	343616.997106	49.169421
3504.062206	343596.457717	49.174426
3504.283789	343576.466796	49.179431
3504.023326	343587.122301	49.184436
3504.452706	343571.603878	49.189441
3504.647027	343579.692994	49.194445
3503.984588	343576.514184	49.199450
3504.168143	343575.721566	49.204455
3504.189213	343580.529056	49.209460
3503.902570	343582.356174	49.214465
3503.967417	343583.185923	49.219469
3503.741971	343572.276380	49.224474
3504.127611	343584.611515	49.229479
3503.782940	343577.997089	49.234484
3504.086869	343582.505319	49.239489
3504.203702	343585.184990	49.244493
3504.021064	343593.180977	49.249498
3504.099921	343587.899560	49.254503
3503.956567	343589.907655	49.259508
3503.911251	343575.635164	49.264513
3503.922915	343579.578707	49.269517
3504.102189	343589.681064	49.274522
3504.044067	343587.883042	49.279527
3503.768568	343596.759145	49.284532
3503.864021	343586.486128	49.289537
3504.065750	343588.388757	49.294541
3503.634081	343598.333162	49.299546
3504.066785	343587.854102	49.304551
3503.954048	343591.970035	49.309556
3504.134744	343588.581565	49.314561
3504.111101	343590.596188	49.319565
3504.239466	343589.659571	49.324570
3504.280050	343593.242185	49.329575
3503.707334	343583.863877	49.334580
3504.181464	343589.974252	49.339585
3504.357369	343586.917441	49.344589
3504.182338	343578.978043	49.349594
3503.927294	343558.120673	49.354599
3503.943869	343570.997786	49.359604
3503.814009	343562.007630	49.364609
3503.632565	343565.676256	49.369613
3503.657872	343593.035294	49.374618
3504.296318	343595.810675	49.379623
3503.960239	343612.078002	49.384628
3504.104609	343600.117292	49.389633
3504.169985	343606.445013	49.394637
3503.772340	343584.362954	49.399642
3504.495831	343576.688763	49.404647
3504.119106	343576.442896	49.409652
3504.371778	343564.770504	49.414657
3504.239291	343570.467708	49.419661
3504.344436	343560.625871	49.424666
3504.650011	343572.719127	49.429671
3504.272566	343575.451489	49.434676
3504.154520	343558.008746	49.439681
3504.098383	343543.127063	49.444685
3504.138501	343546.786115	49.449690
3504.351524	343538.505367	49.454695
3504.259527	343531.978257	49.459700
3504.374640	343530.967374	49.464705
3503.894665	343530.966916	49.469709
3503.934615	343534.880536	49.474714
3504.482326	343531.535854	49.479719
3504.303470	343545.767476	49.484724
3504.475391	343536.780514	49.489729
3504.402071	343517.701633	49.494733
3504.336178	343506.894123	49.499738
3504.016850	343497.781189	49.504743
3504.131830	343506.417392	49.509748
3504.203919	343498.795270	49.514753
3504.203757	343505.540627	49.519757
3504.015752	343515.370161	49.524762
3504.334608	343501.040077	49.529767
3504.129756	343508.683232	49.534772
3504.358231	343504.701761	49.539777
3504.324560	343506.794334	49.544781
3504.153550	343487.094538	49.549786
3504.318361	343479.432299	49.554791
3504.213729	343475.045318	49.559796
3504.145228	343468.819936	49.564801
3504.255741	343474.147828	49.569805
3503.728879	343468.351268	49.574810
3504.450137	343456.502956	49.579815
3504.189227	343474.132953	49.584820
3504.341198	343461.992836	49.589825
3504.289991	343467.982647	49.594829
3504.001496	343470.726405	49.599834
3504.408326	343479.927367	49.604839
3503.938675	343463.023812	49.609844
3504.198708	343452.164763	49.614849
3503.790457	343451.822064	49.619853
3503.890428	343442.261020	49.624858
3504.328065	343442.573661	49.629863
3503.886012	343448.727083	49.634868
3504.149168	343440.692935	49.639873
3504.134421	343457.571306	49.644877
3504.209382	343448.116033	49.649882
3504.289024	343447.314388	49.654887
3504.082117	343458.699615	49.659892
3504.558294	343440.297456	49.664897
3504.533344	343451.221199	49.669901
3504.099890	343437.417304	49.674906
3504.104881	343422.500473	49.679911
3504.334912	343424.347725	49.684916
3504.213922	343409.476262	49.689921
3504.019479	343419.612278	49.694925
3504.167594	343414.574437	49.699930
3504.142667	343412.236627	49.704935
3503.994113	343425.903499	49.709940
3504.155190	343424.528990	49.714945
3504.029061	343424.370773	49.719949
3503.900053	343422.278506	49.724954
3504.494423	343414.370168	49.729959
3504.463473	343419.898608	49.734964
3504.280373	343419.774853	49.739969
3504.092844	343423.215363	49.744973
3504.280677	343402.084289	49.749978
3504.124805	343386.531076	49.754983
3503.812944	343394.445703	49.759988
3504.150259	343387.417986	49.764993
3503.891217	343389.622555	49.769997
3504.141856	343381.030389	49.775002
3504.107060	343379.788663	49.780007
3504.047899	343394.052306	49.785012
3504.097656	343386.255522	49.790017
3504.282043	343382.942818	49.795021
3504.224105	343385.904670	49.800026
3504.518138	343383.363707	49.805031
3504.055752	343388.833090	49.810036
3504.400734	343386.564067	49.815041
3504.326222	343388.815825	49.820045
3504.224547	343382.468408	49.825050
3504.227201	343351.566782	49.830055
3503.871721	343352.513896	49.835060
3504.348989	343351.980288	49.840065
3504.330654	343356.030405	49.845069
3504.473351	343357.942374	49.850074
3504.477722	343350.890928	49.855079
3504.115395	343358.431728	49.860084
3504.147983	343347.048630	49.865089
3504.188681	343343.529555	49.870093
3504.314307	343327.219108	49.875098
3504.676176	343316.369389	49.880103
3504.271087	343325.087841	49.885108
3504.475250	343316.375743	49.890113
3504.370234	343319.497765	49.895117
3504.147629	343321.289311	49.900122
3504.187266	343290.407260	49.905127
3503.964061	343287.438987	49.910132
3504.226135	343277.266845	49.915137
3504.084878	343269.169341	49.920141
3503.883804	343283.684533	49.925146
3504.058726	343278.336993	49.930151
3504.113319	343283.368294	49.935156
3504.094186	343282.327722	49.940161
3503.990337	343292.500345	49.945165
3504.230990	343287.702404	49.950170
3504.372594	343291.269065	49.955175
3503.876231	343287.758533	49.960180
3504.117871	343277.055085	49.965185
3504.209503	343288.316784	49.970189
3504.105778	343287.595035	49.975194
3504.232133	343281.517005	49.980199
3503.962315	343288.712285	49.985204
3504.098566	343287.163519	49.990209
3504.423163	343294.366638	49.995213
3503.989481	343292.246172	50.000218
3504.622432	343261.779386	50.005223
3503.839509	343267.324910	50.010228
3503.676468	343254.445477	50.015233
3503.786749	343264.533342	50.020237
3503.738854	343257.948323	50.025242
3503.880140	343273.962091	50.030247
3503.958069	343292.760368	50.035252
3504.056359	343293.304839	50.040257
3504.246161	343303.201947	50.045261
3504.016543	343277.198735	50.050266
3504.231157	343272.175822	50.055271
3504.023375	343272.921409	50.060276
3504.168895	343262.996778	50.065281
3504.391306	343258.125356	50.070285
3504.049467	343270.524661	50.075290
3504.014061	343256.352345	50.080295
3503.951138	343263.718550	50.085300
3503.927225	343276.220315	50.090305
3504.069100	343266.779889	50.095309
3503.828866	343273.868677	50.100314
3504.195784	343266.072642	50.105319
3503.871808	343277.858223	50.110324
3503.907673	343275.994425	50.115329
3503.840643	343266.281577	50.120333
3503.845687	343280.255101	50.125338
3504.035010	343265.054548	50.130343
3503.678466	343273.281704	50.135348
3503.997606	343266.078667	50.140353
3504.122836	343273.669666	50.145357
3503.949324	343274.766191	50.150362
3504.259532	343272.909928	50.155367
3504.196287	343271.316339	50.160372
3504.073849	343273.753857	50.165377
3504.251849	343270.671245	50.170381
3503.911728	343279.837606	50.175386
3503.844284	343279.568295	50.180391
3503.889675	343287.833721	50.185396
3504.277208	343275.885410	50.190401
3503.848698	343283.563953	50.195405
3503.759401	343288.694365	50.200410
3504.172863	343280.916428	50.205415
3504.198784	343281.523249	50.210420
3504.341379	343288.627872	50.215425
3504.278660	343280.568861	50.220429
3504.201822	343280.046495	50.225434
3504.464514	343289.092096	50.230439
3503.851046	343269.029461	50.235444
3504.637985	343250.247209	50.240449
3504.311767	343254.091467	50.245453
3504.425142	343249.415462	50.250458
3504.095407	343247.253106	50.255463
3504.226817	343246.112371	50.260468
3503.963038	343247.935883	50.265473
3504.050275	343252.631122	50.270477
3504.154335	343253.251044	50.275482
3504.322518	343246.148233	50.280487
3504.224018	343259.552688	50.285492
3504.204213	343240.007085	50.290497
3504.055247	343228.474489	50.295501
3504.084105	343217.702854	50.300506
3504.490675	343223.518499	50.305511
3504.025960	343224.330161	50.310516
3503.832890	343218.531713	50.315521
3503.744030	343220.480296	50.320525
3504.008166	343222.296708	50.325530
3504.274778	343217.214662	50.330535
3504.093236	343225.439611	50.335540
3504.141761	343225.177420	50.340545
3504.218984	343225.521589	50.345549
3503.965664	343237.321462	50.350554
3504.378684	343218.878312	50.355559
3503.838558	343229.399916	50.360564
3503.957891	343223.882981	50.365569
3503.852377	343224.612399	50.370573
3504.169388	343217.486055	50.375578
3504.450507	343218.765246	50.380583
3504.045552	343239.879845	50.385588
3504.064014	343219.666378	50.390593
3504.203581	343226.949666	50.395597
3503.810540	343222.455540	50.400602
3504.154657	343215.197640	50.405607
3503.945498	343215.510724	50.410612
3503.922304	343200.471023	50.415617
3504.011379	343206.158686	50.420621
3503.916464	343208.464585	50.425626
3503.758582	343226.816535	50.430631
3504.071832	343232.316030	50.435636
3504.110386	343221.339230	50.440641
3503.963995	343234.878532	50.445645
3504.145213	343220.621051	50.450650
3504.125453	343211.715253	50.455655
3503.875470	343204.602187	50.460660
3504.233668	343190.494897	50.465665
3504.082102	343189.831619	50.470669
3504.405763	343190.264098	50.475674
3504.141480	343195.371274	50.480679
3503.984645	343206.468637	50.485684
3504.014748	343188.773278	50.490689
3504.074752	343195.050983	50.495693
3503.779437	343203.090291	50.500698
3504.310255	343191.959297	50.505703
3504.459423	343196.033850	50.510708
3504.114776	343195.681094	50.515713
3504.118955	343207.185720	50.520717
3503.828922	343199.035366	50.525722
3503.979870	343197.891541	50.530727
3503.969475	343181.093477	50.535732
3503.996399	343158.765958	50.540737
3503.996260	343132.726403	50.545741
3503.407782	343101.256297	50.550746
3503.875451	343049.764932	50.555751
3503.544315	342999.341619	50.560756
3503.379637	342946.117436	50.565761
3503.117685	342870.228835	50.570765
3502.593629	342802.246957	50.575770
3502.545926	342718.535278	50.580775
3501.759568	342636.722072	50.585780
3501.655914	342540.164537	50.590785
3501.575093	342436.094178	50.595789
3501.044828	342335.963781	50.600794
3500.491891	342212.876810	50.605799
3499.936565	342104.120905	50.610804
3500.126942	341984.657782	50.615809
3499.261117	341863.935952	50.620813
3498.820063	341745.794020	50.625818
3498.621558	341614.097022	50.630823
3497.877947	341480.780451	50.635828
3497.663322	341343.281720	50.640833
3496.790588	341202.195763	50.645837
3496.249536	341058.613365	50.650842
3495.892103	340927.780052	50.655847
3495.462681	340783.848457	50.660852
3495.271475	340631.656841	50.665857
3494.516904	340475.302898	50.670861
3493.739778	340321.014013	50.675866
3493.125541	340156.720486	50.680871
3492.541248	340015.077146	50.685876
3492.172589	339855.300534	50.690881
3491.970429	339701.453798	50.695885
3491.188063	339540.647215	50.700890
3490.679183	339367.883720	50.705895
3489.764504	339200.376893	50.710900
3489.329723	339024.927902	50.715905
3488.712566	338861.318806	50.720909
3488.217607	338694.558891	50.725914
3488.054967	338504.148258	50.730919
3487.044432	338347.778661	50.735924
3486.189896	338167.277032	50.740929
3485.481464	337988.966496	50.745933
3484.657473	337816.986910	50.750938
3484.146154	337646.077517	50.755943
3483.389176	337478.999531	50.760948
3483.016715	337290.400488	50.765953
3482.366752	337123.024659	50.770957
3481.568162	336959.821339	50.775962
3481.300057	336761.098004	50.780967
3480.063080	336596.537530	50.785972
3479.902003	336406.935203	50.790977
3479.410715	336235.306221	50.795981
3478.430493	336058.306312	50.800986
3477.852179	335869.939461	50.805991
3477.156571	335703.763785	50.810996
3476.669393	335514.592367	50.816001
3475.812024	335339.760475	50.821005
3474.877792	335164.278398	50.826010
3474.652175	334988.734745	50.831015
3473.927650	334802.806516	50.836020
3473.228166	334621.761670	50.841025
3472.452905	334441.568430	50.846029
3471.645753	334258.070270	50.851034
3471.321686	334076.811897	50.856039
3470.356765	333904.437315	50.861044
3469.971078	333715.804991	50.866049
3469.495104	333536.784070	50.871053
3468.352728	333353.743868	50.876058
3468.099054	333161.550527	50.881063
3467.355532	332995.655974	50.886068
3466.744186	332800.132279	50.891073
3465.708987	332625.372619	50.896077
3465.398306	332432.677159	50.901082
3464.625597	332259.402601	50.906087
3463.553770	332083.501786	50.911092
3462.830419	331904.719549	50.916097
3462.382575	331713.978703	50.921101
3461.134528	331545.080089	50.926106
3461.063290	331352.267517	50.931111
3459.907148	331190.838407	50.936116
3459.509721	331006.834309	50.941121
3458.838056	330833.514922	50.946125
3458.016083	330661.288169	50.951130
3457.932284	330482.477714	50.956135
3456.912546	330309.594023	50.961140
3456.554295	330127.949240	50.966145
3455.791528	329947.259049	50.971149
3454.900746	329774.811997	50.976154
3454.639814	329590.528225	50.981159
3453.538937	329410.934040	50.986164
3453.052495	329235.926807	50.991169
3452.181265	329059.070553	50.996173
3451.614135	328881.045587	51.001178
3450.884998	328702.332954	51.006183
3450.189229	328534.765955	51.011188
3449.572908	328340.631557	51.016193
3449.038650	328163.185305	51.021197
3448.219221	327989.730013	51.026202
3447.757744	327804.633487	51.031207
3446.938411	327621.604443	51.036212
3446.231293	327447.977429	51.041217
3445.599735	327275.076426	51.046221
3444.684745	327099.139188	51.051226
3444.387051	326918.979403	51.056231
3443.074854	326748.730893	51.061236
3442.622281	326560.880340	51.066241
3442.111511	326392.592089	51.071245
3441.251923	326229.068815	51.076250
3440.834902	326051.573827	51.081255
3440.340455	325879.972067	51.086260
3439.612801	325690.940879	51.091265
3438.719517	325514.920357	51.096269
3437.917585	325338.986853	51.101274
3437.547112	325155.193766	51.106279
3436.681435	324988.359070	51.111284
3436.146328	324809.148723	51.116289
3435.424954	324647.153539	51.121293
3434.927287	324460.323715	51.126298
3434.408816	324277.952438	51.131303
3433.408410	324104.415571	51.136308
3432.753370	323935.101199	51.141313
3432.021964	323754.977573	51.146317
3431.404519	323582.219294	51.151322
3430.844043	323394.276746	51.156327
3429.845270	323251.673300	51.161332
3429.438887	323058.129620	51.166337
3428.981087	322878.291877	51.171341
3427.924116	322708.071094	51.176346
3427.487197	322523.671710	51.181351
3426.713011	322366.874682	51.186356
3426.021366	322188.880260	51.191361
3425.611239	322009.847954	51.196365
3424.845604	321840.114103	51.201370
3424.666902	321653.482347	51.206375
3423.837706	321481.873689	51.211380
3422.841169	321305.758949	51.216385
3422.201424	321117.773110	51.221389
3421.285188	320947.781291	51.226394
3420.824515	320766.055505	51.231399
3419.800206	320591.777022	51.236404
3419.292075	320424.062193	51.241409
3418.572386	320254.012527	51.246413
3417.681512	320080.883225	51.251418
3417.588637	319903.960839	51.256423
3416.643143	319740.591580	51.261428
3416.268209	319571.861099	51.266433
3415.761238	319384.792798	51.271437
3414.739893	319213.643110	51.276442
3414.581586	319018.803817	51.281447
3413.761600	318863.561174	51.286452
3413.058162	318685.307124	51.291457
3412.390671	318509.236842	51.296461
3411.612500	318339.753110	51.301466
3410.994760	318153.769318	51.306471
3410.160209	317980.983710	51.311476
3409.176847	317801.448213	51.316481
3408.614355	317628.695340	51.321485
3407.857954	317464.655680	51.326490
3407.427903	317276.272466	51.331495
3406.515689	317117.986032	51.336500
3406.038907	316946.924421	51.341505
3405.411963	316767.381585	51.346509
3404.529458	316606.899806	51.351514
3404.383353	316421.296467	51.356519
3403.446557	316247.429057	51.361524
3402.758847	316081.313718	51.366529
3402.167155	315907.543926	51.371533
3401.515139	315733.299571	51.376538
3401.041850	315553.832119	51.381543
3399.880965	315394.181799	51.386548
3399.171044	315210.778869	51.391553
3398.876890	315034.286871	51.396557
3397.880459	314860.222817	51.401562
3397.457141	314690.651290	51.406567
3396.618390	314528.784283	51.411572
3395.832809	314349.924330	51.416577
3395.288224	314172.171830	51.421581
3394.373949	314011.487304	51.426586
3394.123413	313847.590982	51.431591
3393.538666	313671.550071	51.436596
3392.591889	313495.948083	51.441601
3392.162256	313320.875160	51.446605
3391.251707	313152.065757	51.451610
3390.668237	312969.708430	51.456615
3390.048187	312811.318274	51.461620
3389.238450	312632.000928	51.466625
3389.074650	312460.042133	51.471629
3387.680766	312294.923757	51.476634
3387.088503	312115.851288	51.481639
3386.772067	311947.378974	51.486644
3386.181272	311790.001304	51.491649
3385.309788	311618.076738	51.496653
3384.477020	311450.423804	51.501658
3384.147174	311277.114381	51.506663
3383.116006	311106.793091	51.511668
3382.638830	310930.196063	51.516673
3382.019699	310764.188996	51.521677
3381.284338	310586.155333	51.526682
3380.734825	310413.465039	51.531687
3380.120733	310252.422044	51.536692
3379.306791	310085.247984	51.541697
3378.826826	309912.902462	51.546701
3377.682915	309743.590140	51.551706
3377.271172	309566.675138	51.556711
3376.434128	309405.589862	51.561716
3375.840924	309236.215195	51.566721
3375.130313	309055.348727	51.571725
3374.298652	308900.602688	51.576730
3373.971670	308726.779777	51.581735
3372.937048	308576.929238	51.586740
3372.289470	308397.477872	51.591745
3372.272011	308234.122374	51.596749
3371.210556	308073.987586	51.601754
3370.841025	307896.070363	51.606759
3370.107940	307727.912615	51.611764
3369.520829	307555.020497	51.616769
3368.540133	307383.922027	51.621773
3367.815749	307220.218651	51.626778
3367.158345	307052.557353	51.631783
3366.314419	306886.911633	51.636788
3365.812131	306730.863044	51.641793
3365.148174	306559.305947	51.646797
3364.229443	306396.294374	51.651802
3363.851734	306222.628869	51.656807
3363.256356	306057.910485	51.661812
3362.610067	305899.871919	51.666817
3361.891965	305732.371338	51.671821
3361.103424	305564.652501	51.676826
3360.708130	305391.854535	51.681831
3359.974286	305227.462629	51.686836
3359.416316	305065.232758	51.691841
3358.654742	304888.137460	51.696845
3357.622638	304730.897070	51.701850
3357.449677	304548.385907	51.706855
3356.807081	304389.835708	51.711860
3356.081795	304228.242510	51.716865
3355.448986	304061.795990	51.721869
3354.634061	303888.196699	51.726874
3354.122179	303721.603330	51.731879
3352.925927	303550.177616	51.736884
3352.297095	303387.167593	51.741889
3352.009077	303217.329528	51.746893
3350.986314	303060.493291	51.751898
3350.872018	302896.688298	51.756903
3350.012060	302730.352589	51.761908
3349.383849	302553.844525	51.766913
3348.620600	302389.454035	51.771917
3347.859066	302229.392346	51.776922
3347.443287	302047.451268	51.781927
3346.864292	301878.803698	51.786932
3345.732175	301719.767810	51.791937
3345.298647	301544.602974	51.796941
3344.433108	301396.220435	51.801946
3343.624283	301221.674858	51.806951
3343.208767	301055.088788	51.811956
3342.429481	300893.042165	51.816961
3342.119004	300719.537741	51.821965
3341.166474	300561.465483	51.826970
3340.795310	300382.418614	51.831975
3339.917558	300222.398749	51.836980
3339.181038	300067.296897	51.841985
3338.986838	299894.384408	51.846989
3337.914884	299731.109605	51.851994
3337.527416	299557.285075	51.856999
3336.643765	299392.401233	51.862004
3336.483850	299229.822092	51.867009
3335.626876	299059.127316	51.872013
3335.145820	298883.075841	51.877018
3334.375477	298712.596225	51.882023
3333.496399	298537.676961	51.887028
3332.679512	298374.207736	51.892033
3332.441520	298199.110340	51.897037
3331.293426	298034.929189	51.902042
3330.486048	297865.880766	51.907047
3329.988813	297701.800104	51.912052
3329.101022	297534.470375	51.917057
3328.375922	297370.349061	51.922061
3327.798531	297205.083694	51.927066
3327.418059	297035.814191	51.932071
3326.634897	296890.496254	51.937076
3325.870425	296713.723512	51.942081
3325.503059	296551.021993	51.947085
3324.801841	296385.342566	51.952090
3324.441000	296217.164323	51.957095
3322.984958	296058.047181	51.962100
3322.671568	295883.392511	51.967105
3322.256969	295723.091690	51.972109
3321.330242	295567.048358	51.977114
3321.103246	295393.576557	51.982119
3319.950513	295225.268073	51.987124
3319.081289	295061.371370	51.992129
3318.528525	294895.972851	51.997133
3317.905935	294733.233841	52.002138
3317.080004	294560.365431	52.007143
3316.239674	294419.384201	52.012148
3315.662683	294249.837848	52.017153
3315.242169	294085.334609	52.022157
3314.056499	293935.570531	52.027162
3314.018003	293772.101729	52.032167
3313.345142	293615.762146	52.037172
3312.921475	293452.277634	52.042177
3311.967867	293284.878448	52.047181
3310.647906	293120.414909	52.052186
3310.503216	292958.745042	52.057191
3309.565017	292812.048112	52.062196
3309.038014	292635.361759	52.067201
3308.749509	292475.267827	52.072205
3307.400186	292328.304555	52.077210
3307.547128	292160.577685	52.082215
3306.770414	292000.662537	52.087220
3305.805419	291841.159082	52.092225
3305.414611	291681.386427	52.097229
3304.514497	291519.809632	52.102234
3303.856435	291339.246542	52.107239
3303.251882	291198.353431	52.112244
3302.400260	291039.417299	52.117249
3301.864704	290869.454514	52.122253
3301.091119	290725.608173	52.127258
3300.601557	290545.705514	52.132263
3299.989246	290393.327277	52.137268
3299.295003	290226.750927	52.142273
3298.627695	290070.306377	52.147277
3297.959433	289898.963256	52.152282
3297.417136	289729.815803	52.157287
3296.861278	289584.992125	52.162292
3296.268559	289408.619611	52.167297
3296.007124	289258.502834	52.172301
3294.714706	289085.271478	52.177306
3294.332757	288913.398603	52.182311
3293.659816	288751.071171	52.187316
3292.950681	288581.338230	52.192321
3292.310857	288410.346308	52.197325
3291.530558	288252.874497	52.202330
3290.627555	288078.231184	52.207335
3290.292441	287922.191397	52.212340
3289.376023	287760.971630	52.217345
3289.171751	287588.407770	52.222349
3288.041624	287436.619324	52.227354
3287.444032	287265.187174	52.232359
3286.919154	287108.081909	52.237364
3286.099229	286939.027824	52.242369
3285.351611	286767.313550	52.247373
3284.498152	286613.876502	52.252378
3284.281527	286444.955965	52.257383
3283.277854	286295.923049	52.262388
3282.431281	286136.474261	52.267393
3282.078125	285969.459746	52.272397
3281.115717	285818.917504	52.277402
3280.504612	285644.124961	52.282407
3279.686636	285499.850366	52.287412
3279.023245	285337.647196	52.292417
3278.452737	285183.095170	52.297421
3277.765114	285021.150393	52.302426
3277.562874	284861.268094	52.307431
3276.662014	284723.780868	52.312436
3275.946052	284545.693604	52.317441
3275.358258	284387.807706	52.322445
3274.395419	284229.828275	52.327450
3273.779559	284070.469557	52.332455
3273.473493	283909.482752	52.337460
3272.779774	283751.791677	52.342465
3271.807635	283590.961073	52.347469
3271.249455	283443.563078	52.352474
3270.740432	283277.641879	52.357479
3270.001261	283128.489652	52.362484
3269.540358	282963.222917	52.367489
3268.833764	282799.930584	52.372493
3267.735994	282646.556295	52.377498
3267.604377	282484.064301	52.382503
3266.681933	282328.471923	52.387508
3265.911532	282167.583524	52.392513
3265.445749	281994.651341	52.397517
3264.390400	281847.458926	52.402522
3264.249689	281673.609310	52.407527
3263.295350	281532.436828	52.412532
3262.556155	281362.018155	52.417537
3262.064717	281204.090647	52.422541
3261.337454	281048.925520	52.427546
3261.013511	280886.794646	52.432551
3260.132893	280727.629722	52.437556
3259.449134	280565.657576	52.442561
3258.746194	280407.610554	52.447565
3257.865087	280261.154308	52.452570
3257.245905	280087.481895	52.457575
3256.298596	279931.969343	52.462580
3256.214232	279775.861816	52.467585
3255.513099	279628.307327	52.472589
3254.606645	279453.661511	52.477594
3254.089350	279307.937082	52.482599
3253.487950	279143.812320	52.487604
3252.875964	278985.674273	52.492609
3252.046853	278818.962250	52.497613
3251.245061	278668.698445	52.502618
3250.866260	278505.506180	52.507623
3250.281448	278348.331553	52.512628
3249.204794	278187.108845	52.517633
3248.901804	278022.834861	52.522637
3248.138836	277880.409093	52.527642
3247.453092	277716.526722	52.532647
3246.404984	277552.319639	52.537652
3245.968981	277394.739357	52.542657
3245.277977	277238.218143	52.547661
3244.301025	277090.681560	52.552666
3243.695491	276931.014194	52.557671
3243.203942	276784.699690	52.562676
3242.353302	276628.713065	52.567681
3242.146394	276473.515985	52.572685
3241.093225	276324.590666	52.577690
3240.467011	276167.371506	52.582695
3239.783171	276025.187810	52.587700
3239.470399	275859.438079	52.592705
3238.717618	275701.041920	52.597709
3237.707554	275558.502337	52.602714
3237.557918	275396.368775	52.607719
3236.630138	275240.419800	52.612724
3235.965930	275091.152783	52.617729
3235.424313	274929.616078	52.622733
3234.881557	274771.696069	52.627738
3234.165771	274625.799051	52.632743
3233.451701	274464.111365	52.637748
3232.757568	274311.818368	52.642753
3232.345894	274147.001180	52.647757
3231.336262	274012.687857	52.652762
3230.921466	273831.240326	52.657767
3229.999000	273683.032962	52.662772
3229.080189	273515.469061	52.667777
3228.360442	273367.458863	52.672781
3228.048810	273214.494179	52.677786
3227.382716	273062.502450	52.682791
3226.613125	272907.700122	52.687796
3226.069336	272749.525727	52.692801
3225.303909	272601.624700	52.697805
3224.306368	272455.364918	52.702810
3223.975482	272302.683526	52.707815
3223.506410	272153.869737	52.712820
3222.814850	271987.085042	52.717825
3222.162370	271832.111502	52.722829
3221.035496	271693.945744	52.727834
3220.845636	271520.536378	52.732839
3220.135224	271375.428320	52.737844
3219.194900	271212.299611	52.742849
3218.869742	271061.018247	52.747853
3217.585189	270923.004889	52.752858
3217.471947	270751.035237	52.757863
3216.420186	270616.015827	52.762868
3215.635319	270457.446959	52.767873
3215.207926	270312.778197	52.772877
3214.328525	270171.772008	52.777882
3213.990608	270016.596204	52.782887
3213.133643	269872.402986	52.787892
3212.535756	269717.115568	52.792897
3212.285040	269559.277365	52.797901
3211.353382	269423.959018	52.802906
3210.491529	269267.720205	52.807911
3209.612335	269120.168852	52.812916
3209.400213	268964.820575	52.817921
3208.853355	268818.337314	52.822925
3208.459174	268657.949738	52.827930
3207.611562	268497.761289	52.832935
3206.500107	268347.750986	52.837940
3205.947022	268188.101793	52.842945
3205.413734	268041.820327	52.847949
3204.483530	267901.866882	52.852954
3203.821798	267737.192306	52.857959
3203.345904	267602.617254	52.862964
3202.667980	267434.838217	52.867969
3202.200341	267295.932348	52.872973
3201.182834	267153.828126	52.877978
3200.821710	266984.241813	52.882983
3200.138038	266847.815198	52.887988
3199.154348	266693.455579	52.892993
3198.863174	266539.164717	52.897997
3198.090846	266385.026442	52.903002
3197.764069	266231.276150	52.908007
3197.200487	266078.174614	52.913012
3196.388849	265922.667444	52.918017
3195.512748	265776.873875	52.923021
3194.672515	265616.328661	52.928026
3194.042950	265469.604809	52.933031
3193.233473	265308.341743	52.938036
3192.523936	265162.165487	52.943041
3191.964086	265019.785809	52.948045
3191.295932	264858.042142	52.953050
3190.886026	264720.324968	52.958055
3190.132527	264576.065993	52.963060
3189.434305	264416.542992	52.968065
3188.758349	264257.220281	52.973069
3187.772355	264115.290395	52.978074
3187.700944	263962.952258	52.983079
3186.989698	263809.365626	52.988084
3186.029795	263667.508197	52.993089
3185.478499	263506.561620	52.998093
3184.642598	263361.552141	53.003098
3184.119542	263198.665681	53.008103
3183.190002	263054.817209	53.013108
3182.541531	262912.961758	53.018113
3181.881833	262767.389835	53.023117
3180.919841	262622.477040	53.028122
3180.637917	262474.986321	53.033127
3179.887094	262333.682151	53.038132
3179.521137	262182.843111	53.043137
3178.368758	262036.177968	53.048141
3177.587935	261897.629271	53.053146
3177.136182	261742.983856	53.058151
3176.613515	261611.601831	53.063156
3176.186472	261448.420951	53.068161
3175.582752	261305.413118	53.073165
3174.638826	261154.564187	53.078170
3174.396358	261000.089794	53.083175
3173.433726	260855.610916	53.088180
3172.450687	260706.882236	53.093185
3172.158773	260556.974633	53.098189
3171.072282	260417.379915	53.103194
3170.435175	260260.294278	53.108199
3170.083831	260122.544397	53.113204
3169.236888	259976.214012	53.118209
3169.022557	259839.435837	53.123213
3168.057457	259691.850928	53.128218
3167.604986	259536.468306	53.133223
3166.828752	259386.052252	53.138228
3166.239594	259244.927815	53.143233
3165.588658	259077.428852	53.148237
3164.827750	258935.847884	53.153242
3164.311327	258780.017436	53.158247
3163.562665	258638.740313	53.163252
3163.015872	258483.704353	53.168257
3162.353770	258335.664828	53.173261
3161.384073	258190.730163	53.178266
3160.975054	258029.229434	53.183271
3160.111456	257888.760437	53.188276
3159.289321	257737.614121	53.193281
3158.606587	257593.856856	53.198285
3157.981439	257450.166972	53.203290
3157.272227	257310.106846	53.208295
3156.719162	257158.969274	53.213300
3155.933681	257011.994289	53.218305
3155.502344	256861.729014	53.223309
3154.394934	256732.071993	53.228314
3154.227034	256577.130181	53.233319
3153.392976	256447.251805	53.238324
3152.326374	256294.107782	53.243329
3151.941093	256154.481019	53.248333
3151.319437	256017.489408	53.253338
3150.769723	255865.715534	53.258343
3150.267235	255733.467616	53.263348
3149.489983	255575.974382	53.268353
3148.744592	255428.000934	53.273357
3148.041235	255288.577893	53.278362
3147.654794	255128.119912	53.283367
3146.814945	254988.871481	53.288372
3146.110619	254847.793541	53.293377
3145.624748	254695.424701	53.298381
3144.787227	254557.067554	53.303386
3144.082354	254406.159750	53.308391
3143.511855	254268.346295	53.313396
3142.739085	254117.322127	53.318401
3142.246645	253962.993949	53.323405
3141.646597	253833.538642	53.328410
3140.843866	253688.988156	53.333415
3140.301901	253538.742869	53.338420
3139.486412	253392.182750	53.343425
3138.683874	253251.758207	53.348429
3137.911768	253096.634600	53.353434
3137.433829	252960.564674	53.358439
3136.570114	252822.416690	53.363444
3135.789196	252682.549437	53.368449
3135.163517	252526.664613	53.373453
3134.133226	252399.137483	53.378458
3133.900825	252250.295882	53.383463
3133.417603	252113.463440	53.388468
3132.765556	251970.545823	53.393473
3132.012128	251839.308090	53.398477
3131.060089	251695.623243	53.403482
3130.830774	251558.445460	53.408487
3130.013326	251421.233529	53.413492
3129.472173	251271.091906	53.418497
3129.036468	251129.490486	53.423501
3127.873327	250984.158861	53.428506
3127.237548	250849.923697	53.433511
3126.818513	250693.753177	53.438516
3126.084076	250573.362144	53.443521
3125.591262	250419.088079	53.448525
3124.570189	250283.997562	53.453530
3124.036743	250129.755670	53.458535
3123.351752	249999.781880	53.463540
3122.683281	249854.831376	53.468545
3122.235915	249702.053321	53.473549
3121.308355	249573.518916	53.478554
3120.834302	249427.901379	53.483559
3120.391737	249282.304460	53.488564
3119.527828	249151.544766	53.493569
3119.023889	249004.124254	53.498573
3118.240284	248871.645854	53.503578
3117.575178	248713.478936	53.508583
3116.929692	248577.082613	53.513588
3116.108799	248435.188028	53.518593
3115.536462	248292.210133	53.523597
3114.665966	248143.855291	53.528602
3114.040840	248001.751873	53.533607
3113.194183	247871.296150	53.538612
3112.767723	247722.693195	53.543617
3112.267406	247588.668606	53.548621
3111.234059	247457.275091	53.553626
3110.963712	247305.108090	53.558631
3110.275732	247174.755207	53.563636
3109.627403	247032.681872	53.568641
3109.042107	246877.993115	53.573645
3108.107009	246747.221347	53.578650
3107.677898	246595.131159	53.583655
3107.197687	246463.956607	53.588660
3106.047676	246308.466545	53.593665
3105.661833	246177.481052	53.598669
3104.654258	246030.983619	53.603674
3104.172461	245891.558978	53.608679
3103.743344	245756.455297	53.613684
3102.530584	245613.836091	53.618689
3102.108359	245468.927349	53.623693
3101.414051	245341.964102	53.628698
3100.997871	245185.391484	53.633703
3100.238675	245061.316375	53.638708
3099.604061	244901.060698	53.643713
3099.071145	244768.801100	53.648717
3098.137900	244630.315035	53.653722
3097.818056	244485.391154	53.658727
3096.886680	244348.483944	53.663732
3096.431290	244216.187166	53.668737
3095.627792	244054.431328	53.673741
3094.803466	243930.520386	53.678746
3094.474636	243772.229450	53.683751
3093.458530	243642.568527	53.688756
3092.644580	243496.679878	53.693761
3092.310962	243358.838763	53.698765
3091.114291	243232.822889	53.703770
3090.827659	243089.092184	53.708775
3090.136607	242964.830043	53.713780
3089.195312	242820.439306	53.718785
3089.055657	242675.641746	53.723789
3088.100804	242543.018320	53.728794
3087.583014	242401.107543	53.733799
3086.969113	242278.005268	53.738804
3086.553753	242126.554708	53.743809
3085.957038	241989.979065	53.748813
3084.746294	241850.852414	53.753818
3084.197176	241708.718217	53.758823
3083.595145	241562.008899	53.763828
3082.598519	241419.920406	53.768833
3082.087563	241278.366368	53.773837
3081.668276	241148.588147	53.778842
3080.924792	241009.057480	53.783847
3080.125305	240882.191770	53.788852
3079.621009	240747.512768	53.793857
3079.241979	240593.792047	53.798861
3078.080010	240456.823801	53.803866
3077.312453	240316.763013	53.808871
3076.630287	240189.828559	53.813876
3076.139526	240048.476527	53.818881
3075.872965	239916.460095	53.823885
3074.812430	239770.233021	53.828890
3074.043315	239645.120905	53.833895
3073.076554	239504.354172	53.838900
3072.581605	239371.254089	53.843905
3072.370726	239240.884809	53.848909
3071.502573	239105.781502	53.853914
3070.783651	238971.189488	53.858919
3070.235796	238834.151462	53.863924
3069.250607	238700.009347	53.868929
3068.640294	238564.713103	53.873933
3068.101814	238432.945165	53.878938
3067.622926	238289.352625	53.883943
3067.024443	238149.955304	53.888948
3066.128973	238024.915938	53.893953
3065.820609	237874.676313	53.898957
3064.853037	237753.442804	53.903962
3064.148837	237615.437956	53.908967
3063.725235	237479.120416	53.913972
3062.755714	237344.544606	53.918977
3062.146759	237202.221826	53.923981
3061.432558	237077.511365	53.928986
3060.755544	236937.262278	53.933991
3059.891442	236804.936741	53.938996
3059.058840	236682.639077	53.944001
3058.706428	236547.075377	53.949005
3058.197494	236423.962875	53.954010
3057.533507	236278.441637	53.959015
3056.991641	236156.276817	53.964020
3056.530281	236007.540942	53.969025
3055.598793	235882.586201	53.974029
3054.723582	235735.138473	53.979034
3054.225524	235595.575847	53.984039
3053.784396	235471.435212	53.989044
3052.673300	235338.717769	53.994049
3052.150980	235202.036882	53.999053
3051.545124	235072.677365	54.004058
3050.872246	234935.664183	54.009063
3050.216796	234792.333552	54.014068
3049.750030	234663.130790	54.019073
3048.875842	234524.240297	54.024077
3048.085056	234412.760573	54.029082
3047.398256	234267.373147	54.034087
3046.759909	234138.325542	54.039092
3046.097133	234004.876871	54.044097
3045.881463	233869.931683	54.049101
3045.098324	233739.990853	54.054106
3044.334702	233594.922139	54.059111
3043.634133	233476.706991	54.064116
3042.841110	233325.990574	54.069121
3042.404051	233202.030377	54.074125
3041.483650	233072.366797	54.079130
3041.185142	232933.667534	54.084135
3040.606821	232807.234859	54.089140
3039.527424	232667.462842	54.094145
3038.937031	232539.250047	54.099149
3038.367780	232399.092123	54.104154
3037.776747	232263.699352	54.109159
3037.006445	232136.355845	54.114164
3036.502314	231998.581686	54.119169
3036.015662	231871.982976	54.124173
3034.933706	231724.854117	54.129178
3034.446618	231588.885695	54.134183
3033.636240	231450.753424	54.139188
3032.924681	231325.438714	54.144193
3032.692799	231183.726936	54.149197
3031.745662	231066.445019	54.154202
3031.161460	230918.245628	54.159207
3030.573859	230786.495562	54.164212
3029.687774	230646.390438	54.169217
3029.246596	230519.964624	54.174221
3028.525014	230377.873295	54.179226
3027.897870	230253.972569	54.184231
3027.527372	230115.849075	54.189236
3026.185013	229978.719877	54.194241
3025.778968	229827.947879	54.199245
3025.131229	229705.782579	54.204250
3024.525060	229571.465585	54.209255
3023.843465	229447.269055	54.214260
3023.228505	229300.553982	54.219265
3022.794647	229169.978657	54.224269
3021.572053	229036.574828	54.229274
3020.899034	228891.881098	54.234279
3019.900898	228761.650321	54.239284
3019.073068	228636.306856	54.244289
3018.789215	228504.995855	54.249293
3018.041323	228369.608292	54.254298
3017.354792	228249.182542	54.259303
3016.701592	228132.850967	54.264308
3016.166301	227997.252105	54.269313
3016.015071	227860.777899	54.274317
3014.978391	227746.340767	54.279322
3014.609663	227593.682589	54.284327
3013.825528	227471.211025	54.289332
3012.893344	227343.416232	54.294337
3012.647447	227202.935205	54.299341
3011.656640	227077.390672	54.304346
3011.388892	226944.297246	54.309351
3010.360820	226814.366978	54.314356
3009.879775	226673.796754	54.319361
3009.390333	226544.698234	54.324365
3008.301365	226423.613152	54.329370
3007.660339	226280.128187	54.334375
3007.288239	226156.460314	54.339380
3006.167142	226023.223378	54.344385
3005.621994	225894.478411	54.349389
3004.948189	225766.174114	54.354394
3004.644267	225635.214479	54.359399
3003.746358	225505.787609	54.364404
3003.083280	225377.558605	54.369409
3002.522048	225240.580728	54.374413
3001.796673	225108.250141	54.379418
3000.922128	224981.099121	54.384423
3000.561350	224855.369131	54.389428
2999.807725	224729.472385	54.394433
2999.260526	224593.842783	54.399437
2998.195609	224467.193730	54.404442
2997.621391	224343.025949	54.409447
2997.103223	224211.733368	54.414452
2996.204050	224079.915737	54.419457
2995.501846	223957.080017	54.424461
2994.712456	223843.385722	54.429466
2994.386836	223699.549890	54.434471
2993.861694	223579.474601	54.439476
2992.878760	223449.759002	54.444481
2992.711990	223323.720667	54.449485
2991.770445	223185.889979	54.454490
2990.780659	223067.836711	54.459495
2990.124186	222937.866604	54.464500
2989.829755	222812.040255	54.469505
2989.257620	222680.389618	54.474509
2988.402637	222556.358225	54.479514
2987.898734	222427.981510	54.484519
2987.110304	222300.362921	54.489524
2986.402928	222170.389439	54.494529
2985.924643	222040.850910	54.499533
2985.335079	221916.816724	54.504538
2984.678267	221778.625240	54.509543
2984.024095	221649.611680	54.514548
2983.299978	221512.411521	54.519553
2982.587134	221392.012931	54.524557
2981.848289	221266.475890	54.529562
2981.276668	221133.478508	54.534567
2980.581263	221004.867199	54.539572
2979.921495	220876.212280	54.544577
2979.136926	220752.860090	54.549581
2978.656727	220623.133360	54.554586
2977.914693	220494.937657	54.559591
2977.374544	220355.686511	54.564596
2976.672581	220223.246028	54.569601
2975.880835	220095.746277	54.574605
2975.136892	219969.843082	54.579610
2974.431762	219839.084072	54.584615
2973.922287	219725.517115	54.589620
2973.318894	219595.557112	54.594625
2972.854150	219464.404295	54.599629
2971.961167	219336.654581	54.604634
2971.398907	219190.802659	54.609639
2970.739616	219072.168743	54.614644
2970.140552	218950.101331	54.619649
2969.879411	218805.284498	54.624653
2968.676502	218664.804946	54.629658
2968.039999	218535.501278	54.634663
2967.476685	218410.094093	54.639668
2966.916788	218282.649933	54.644673
2966.093205	218152.052753	54.649677
2965.452135	218027.180444	54.654682
2964.787586	217890.219507	54.659687
2964.006836	217756.841349	54.664692
2963.238149	217635.299474	54.669697
2962.712713	217503.968925	54.674701
2961.832574	217384.469032	54.679706
2961.013967	217244.504258	54.684711
2960.959819	217121.653631	54.689716
2960.088690	217004.202310	54.694721
2959.231636	216859.789296	54.699725
2958.507204	216739.603957	54.704730
2958.075288	216616.508539	54.709735
2957.427116	216481.138867	54.714740
2956.540272	216366.211411	54.719745
2956.097165	216230.606104	54.724749
2955.583156	216105.844404	54.729754
2954.656273	215980.104548	54.734759
2953.921526	215854.894564	54.739764
2953.278279	215731.541430	54.744769
2952.655175	215605.894183	54.749773
2951.879875	215476.923650	54.754778
2951.277427	215351.349975	54.759783
2950.630837	215220.539369	54.764788
2949.794442	215105.135097	54.769793
2949.287791	214973.029964	54.774797
2948.514570	214850.348167	54.779802
2947.743022	214716.987175	54.784807
2947.517156	214595.326557	54.789812
2946.757812	214471.077662	54.794817
2946.272584	214337.264788	54.799821
2945.367589	214224.876786	54.804826
2944.542768	214097.635069	54.809831
2944.048736	213970.277581	54.814836
2942.946364	213850.309950	54.819841
2942.607039	213717.455302	54.824845
2941.935115	213601.900311	54.829850
2941.552649	213475.468002	54.834855
2940.868414	213348.472762	54.839860
2939.894076	213230.840702	54.844865
2939.427170	213100.667682	54.849869
2938.820183	212980.814129	54.854874
2938.314287	212845.760203	54.859879
2937.702845	212723.260392	54.864884
2937.048180	212589.121517	54.869889
2936.281901	212458.551703	54.874893
2935.615474	212328.450005	54.879898
2935.011594	212193.260218	54.884903
2934.273610	212065.614146	54.889908
2933.247838	211943.219601	54.894913
2932.967789	211798.357088	54.899917
2932.014046	211689.748627	54.904922
2931.477895	211571.108352	54.909927
2931.050909	211433.804799	54.914932
2930.062151	211320.582325	54.919937
2929.454952	211187.329813	54.924941
2928.862904	211076.272318	54.929946
2927.899817	210925.436092	54.934951
2927.491167	210814.922765	54.939956
2927.090783	210695.651705	54.944961
2926.797958	210554.497799	54.949965
2925.627897	210433.236320	54.954970
2925.003746	210298.741069	54.959975
2924.430971	210166.668932	54.964980
2923.645799	210050.425542	54.969985
2923.034771	209919.263639	54.974989
2922.231801	209795.514330	54.979994
2921.521524	209666.137794	54.984999
2920.898277	209542.220533	54.990004
2919.867885	209422.606204	54.995009
2919.761592	209279.758368	55.000013
2918.718787	209167.681093	55.005018
2918.216598	209039.685658	55.010023
2917.424872	208907.727243	55.015028
2916.730999	208789.906319	55.020033
2916.314622	208659.187188	55.025037
2915.655352	208537.224926	55.030042
2915.318003	208414.677395	55.035047
2914.297733	208281.051084	55.040052
2913.284476	208160.011077	55.045057
2913.246111	208037.773326	55.050061
2911.973608	207907.025923	55.055066
2911.344258	207779.893262	55.060071
2911.314415	207659.793069	55.065076
2910.192836	207549.309409	55.070081
2909.565702	207418.206343	55.075085
2908.784752	207294.458633	55.080090
2908.255108	207169.258701	55.085095
2907.712418	207034.363215	55.090100
2906.853270	206923.788252	55.095105
2906.596537	206780.702875	55.100109
2905.806593	206663.715846	55.105114
2905.074821	206535.711179	55.110119
2904.497591	206404.271551	55.115124
2903.673253	206277.351149	55.120129
2902.969471	206148.961088	55.125133
2902.157905	206029.662486	55.130138
2901.469400	205908.232018	55.135143
2901.106751	205786.470220	55.140148
2899.984735	205662.996290	55.145153
2899.521672	205536.656616	55.150157
2898.759085	205427.189118	55.155162
2898.177031	205301.225140	55.160167
2897.991522	205166.862802	55.165172
2896.607143	205050.393102	55.170177
2896.049300	204936.032608	55.175181
2895.377168	204814.296401	55.180186
2894.983511	204679.993608	55.185191
2894.312152	204577.156439	55.190196
2893.066507	204451.146679	55.195201
2892.882025	204325.274595	55.200205
2892.248002	204205.378956	55.205210
2891.506969	204099.053957	55.210215
2890.698687	203957.971796	55.215220
2889.873835	203851.406009	55.220225
2889.657095	203718.630053	55.225229
2888.749882	203616.506450	55.230234
2887.916367	203491.744346	55.235239
2887.543939	203384.242420	55.240244
2886.616749	203263.517095	55.245249
2886.126192	203134.412794	55.250253
2885.438631	203026.108809	55.255258
2885.011688	202909.071926	55.260263
2884.190749	202787.859936	55.265268
2883.658676	202666.513385	55.270273
2883.114462	202537.864361	55.275277
2882.211463	202429.430210	55.280282
2881.314549	202303.637266	55.285287
2880.794640	202180.177359	55.290292
2880.139645	202079.620070	55.295297
2879.472651	201948.981177	55.300301
2879.181993	201829.201668	55.305306
2878.154000	201709.615533	55.310311
2877.656863	201596.804730	55.315316
2877.023178	201471.506474	55.320321
2876.477500	201360.167292	55.325325
2875.484187	201241.976500	55.330330
2874.722916	201121.967639	55.335335
2874.406634	200984.620029	55.340340
2873.594944	200885.858584	55.345345
2873.429990	200759.291532	55.350349
2872.587256	200634.868176	55.355354
2871.906730	200517.278420	55.360359
2871.087796	200386.896368	55.365364
2870.183683	200265.868532	55.370369
2869.841376	200143.530369	55.375373
2869.073727	200037.001043	55.380378
2868.290187	199911.310171	55.385383
2867.951745	199794.405882	55.390388
2866.712007	199678.649867	55.395393
2866.233917	199542.069599	55.400397
2865.689135	199436.969566	55.405402
2864.935498	199316.772623	55.410407
2864.216711	199195.170670	55.415412
2863.521176	199087.232049	55.420417
2863.214919	198959.190040	55.425421
2862.120402	198847.217622	55.430426
2861.454462	198722.032650	55.435431
2861.197941	198610.144352	55.440436
2860.175021	198496.888840	55.445441
2859.573617	198366.693586	55.450445
2858.906685	198261.208025	55.455450
2858.364592	198147.698970	55.460455
2857.633166	198032.145996	55.465460
2857.005048	197909.858221	55.470465
2856.590114	197789.203915	55.475469
2855.419499	197680.439947	55.480474
2855.037844	197555.747166	55.485479
2854.435026	197442.147457	55.490484
2853.682187	197323.354644	55.495489
2853.184402	197199.151918	55.500493
2852.136326	197084.630982	55.505498
2851.654356	196962.169588	55.510503
2851.005780	196857.765542	55.515508
2850.406807	196736.493869	55.520513
2850.155808	196620.040851	55.525517
2849.392760	196505.476058	55.530522
2848.342792	196383.844005	55.535527
2847.982062	196251.923570	55.540532
2847.022874	196136.270917	55.545537
2846.442917	196021.309202	55.550541
2845.735643	195899.980306	55.555546
2844.823936	195791.370178	55.560551
2844.145220	195665.011227	55.565556
2843.287060	195571.789430	55.570561
2843.181234	195434.677423	55.575565
2842.296627	195326.394825	55.580570
2841.752310	195220.132601	55.585575
2841.304487	195098.637284	55.590580
2840.672725	194987.643305	55.595585
2839.870915	194863.596177	55.600589
2839.042033	194754.886084	55.605594
2838.461637	194633.756429	55.610599
2837.806078	194515.603652	55.615604
2837.103215	194398.947344	55.620609
2836.583093	194276.740193	55.625613
2836.333643	194164.885876	55.630618
2835.360476	194050.499865	55.635623
2834.962336	193937.104572	55.640628
2834.377952	193811.396963	55.645633
2833.269764	193676.662425	55.650637
2832.556805	193567.198575	55.655642
2832.039736	193453.556021	55.660647
2831.473343	193327.554141	55.665652
2830.453528	193215.607658	55.670657
2830.313128	193088.928186	55.675661
2829.394760	192971.787686	55.680666
2828.671305	192849.438116	55.685671
2828.164477	192731.584110	55.690676
2827.239678	192607.294887	55.695681
2826.924829	192491.179615	55.700685
2826.013815	192367.321415	55.705690
2825.263260	192244.710453	55.710695
2824.555340	192126.431707	55.715700
2823.507588	192021.184854	55.720705
2822.992735	191899.860654	55.725709
2822.421764	191798.406651	55.730714
2821.381720	191680.881368	55.735719
2821.015366	191571.405244	55.740724
2820.353999	191463.451979	55.745729
2819.917835	191341.964032	55.750733
2818.944396	191237.585007	55.755738
2818.443734	191116.718551	55.760743
2817.719583	191007.427602	55.765748
2817.109480	190897.011935	55.770753
2816.886591	190772.552625	55.775757
2815.958570	190662.671321	55.780762
2815.300704	190551.335237	55.785767
2814.696624	190428.680234	55.790772
2813.661735	190322.239098	55.795777
2813.258405	190204.921926	55.800781
2812.758251	190090.215831	55.805786
2811.954159	189974.922010	55.810791
2811.030895	189863.527783	55.815796
2810.608124	189757.512594	55.820801
2810.026511	189635.937505	55.825805
2809.319834	189520.921980	55.830810
2808.656299	189399.436808	55.835815
2807.895077	189283.756201	55.840820
2807.320355	189175.565373	55.845825
2806.830696	189052.514125	55.850829
2805.791166	188950.071683	55.855834
2805.166704	188828.301900	55.860839
2804.453572	188712.462411	55.865844
2803.564053	188607.032631	55.870849
2803.252722	188494.463313	55.875853
2802.513084	188386.224091	55.880858
2801.838923	188271.499088	55.885863
2801.137220	188166.562170	55.890868
2800.529212	188044.957210	55.895873
2799.971566	187935.379818	55.900877
2798.884501	187828.621809	55.905882
2798.296274	187717.154168	55.910887
2797.937927	187603.805675	55.915892
2797.230869	187503.883626	55.920897
2796.495770	187376.295713	55.925901
2796.126730	187279.157635	55.930906
2795.207227	187160.365019	55.935911
2794.645285	187053.576517	55.940916
2793.918859	186939.181142	55.945921
2793.422924	186823.846289	55.950925
2792.672100	186727.634936	55.955930
2791.874534	186607.666744	55.960935
2791.457776	186498.286723	55.965940
2790.459826	186385.029816	55.970945
2790.021909	186261.990499	55.975949
2789.231858	186143.816105	55.980954
2788.795470	186036.005074	55.985959
2788.104416	185935.091617	55.990964
2787.474717	185825.785103	55.995969
2786.698468	185694.239244	56.000973
2786.095932	185591.391570	56.005978
2785.683834	185481.873316	56.010983
2784.864508	185361.746478	56.015988
2783.863419	185255.833203	56.020993
2783.441846	185138.760721	56.025997
2782.437215	185025.075744	56.031002
2781.837321	184921.389565	56.036007
2780.924940	184799.485251	56.041012
2780.485164	184704.373849	56.046017
2780.107841	184590.425235	56.051021
2779.111724	184487.057246	56.056026
2778.443066	184370.458429	56.061031
2778.265236	184265.549284	56.066036
2777.340007	184162.527013	56.071041
2776.580786	184040.982145	56.076045
2775.853933	183932.408010	56.081050
2775.410776	183821.779275	56.086055
2774.908951	183711.732556	56.091060
2773.815172	183607.962286	56.096065
2773.483552	183492.444557	56.101069
2772.555254	183387.236565	56.106074
2771.727657	183282.280012	56.111079
2771.642944	183168.454066	56.116084
2770.756764	183064.588587	56.121089
2770.360669	182943.434446	56.126093
2769.766159	182835.439924	56.131098
2768.796681	182718.765899	56.136103
2768.543613	182608.886062	56.141108
2767.758652	182491.979883	56.146113
2767.157696	182371.851984	56.151117
2766.212750	182264.385044	56.156122
2765.700355	182148.492422	56.161127
2765.372716	182020.091975	56.166132
2764.252267	181905.504769	56.171137
2763.821105	181789.294943	56.176141
2762.794398	181686.129188	56.181146
2762.309088	181566.799303	56.186151
2761.557514	181455.105995	56.191156
2760.716392	181350.715927	56.196161
2760.320666	181234.692781	56.201165
2759.553896	181129.133921	56.206170
2758.713599	181014.746385	56.211175
2758.110050	180901.123025	56.216180
2757.246287	180797.882704	56.221185
2756.785210	180689.465337	56.226189
2756.071507	180581.813309	56.231194
2755.193853	180467.076986	56.236199
2754.792214	180361.296815	56.241204
2754.014856	180255.550981	56.246209
2753.740716	180141.330495	56.251213
2752.832419	180038.607860	56.256218
2752.169022	179922.401705	56.261223
2751.483749	179814.925187	56.266228
2751.043020	179708.275154	56.271233
2750.252815	179592.598783	56.276237
2749.669727	179489.368048	56.281242
2749.030940	179371.594966	56.286247
2748.637786	179267.393422	56.291252
2747.480029	179168.859047	56.296257
2746.995706	179043.748577	56.301261
2746.254697	178936.855502	56.306266
2745.587414	178829.098807	56.311271
2745.024775	178708.695273	56.316276
2744.214932	178599.664352	56.321281
2743.642585	178488.344741	56.326285
2742.639859	178384.788882	56.331290
2742.145047	178276.853649	56.336295
2741.788551	178167.866513	56.341300
2740.722121	178053.153928	56.346305
2740.257487	177942.085814	56.351309
2739.360811	177840.689513	56.356314
2738.864488	177736.317325	56.361319
2738.501129	177619.586669	56.366324
2737.655709	177521.947921	56.371329
2736.918055	177407.553893	56.376333
2736.155644	177302.499953	56.381338
2735.611372	177194.410014	56.386343
2734.974577	177081.247383	56.391348
2734.044927	176977.899678	56.396353
2734.031221	176851.729143	56.401357
2733.108967	176748.457156	56.406362
2732.625947	176644.632528	56.411367
2732.045528	176546.254566	56.416372
2731.162728	176432.064300	56.421377
2730.598711	176311.349963	56.426381
2729.893138	176199.129128	56.431386
2728.892093	176080.672336	56.436391
2728.224113	175971.613143	56.441396
2727.573985	175879.963316	56.446401
2727.038144	175764.168269	56.451405
2726.496600	175660.775122	56.456410
2725.426658	175552.836373	56.461415
2725.178119	175434.376718	56.466420
2724.576244	175324.736449	56.471425
2723.831805	175208.848842	56.476429
2723.071424	175102.095946	56.481434
2722.431334	174990.898263	56.486439
2721.848520	174874.311933	56.491444
2720.913348	174778.856076	56.496449
2720.656897	174668.018212	56.501453
2720.002960	174547.768496	56.506458
2719.178092	174437.339271	56.511463
2718.589429	174325.257716	56.516468
2718.047762	174225.238585	56.521473
2717.361412	174110.298796	56.526477
2716.315279	174011.479313	56.531482
2715.785033	173894.798466	56.536487
2715.280762	173788.847874	56.541492
2714.647453	173670.568817	56.546497
2714.135600	173554.204000	56.551501
2713.151547	173445.252578	56.556506
2712.301568	173337.882671	56.561511
2711.953959	173227.470204	56.566516
2711.077074	173121.440520	56.571521
2711.000246	173008.925472	56.576525
2709.980254	172898.124447	56.581530
2709.109794	172781.755113	56.586535
2708.851855	172675.094424	56.591540
2707.888472	172566.816179	56.596545
2707.254727	172459.274502	56.601549
2706.603774	172346.508915	56.606554
2706.070081	172236.370325	56.611559
2705.365558	172122.151350	56.616564
2704.373474	172011.704484	56.621569
2704.011904	171894.939211	56.626573
2703.200385	171795.121565	56.631578
2702.275671	171677.772132	56.636583
2702.116030	171566.177252	56.641588
2701.424891	171473.653821	56.646593
2700.800543	171361.942385	56.651597
2700.387168	171245.441602	56.656602
2699.161847	171127.887101	56.661607
2698.520900	171019.434877	56.666612
2698.113596	170908.771313	56.671617
2697.699801	170795.425787	56.676621
2696.679007	170691.015105	56.681626
2696.012443	170581.334609	56.686631
2695.483980	170470.856809	56.691636
2694.768957	170364.503735	56.696641
2694.105663	170248.007386	56.701645
2693.480533	170136.286884	56.706650
2692.829171	170023.629815	56.711655
2692.044558	169911.324824	56.716660
2691.378010	169812.926304	56.721665
2690.776629	169692.784831	56.726669
2690.128174	169583.256905	56.731674
2689.156203	169476.946991	56.736679
2688.752437	169363.476915	56.741684
2687.716705	169253.019393	56.746689
2687.454995	169152.778108	56.751693
2686.814639	169050.409835	56.756698
2686.282159	168939.822622	56.761703
2685.587856	168828.447516	56.766708
2684.808396	168721.549682	56.771713
2684.366006	168597.151902	56.776717
2683.739457	168491.413109	56.781722
2682.969000	168377.152069	56.786727
2682.519020	168258.631521	56.791732
2681.383743	168154.500217	56.796737
2680.994364	168041.807487	56.801741
2680.045466	167931.314617	56.806746
2679.698431	167818.310656	56.811751
2679.097868	167699.523248	56.816756
2678.373531	167602.423918	56.821761
2677.633272	167471.248527	56.826765
2676.909411	167369.686415	56.831770
2676.201918	167257.097293	56.836775
2675.732486	167146.187434	56.841780
2674.815304	167034.013679	56.846785
2674.214536	166917.454045	56.851789
2673.198831	166817.516426	56.856794
2673.002687	166706.857030	56.861799
2672.290809	166589.057167	56.866804
2671.177838	166485.689899	56.871809
2670.645972	166374.906659	56.876813
2670.195239	166274.499514	56.881818
2669.414419	166166.057858	56.886823
2668.986871	166047.426297	56.891828
2668.599916	165951.778229	56.896833
2668.100300	165832.828169	56.901837
2667.167860	165725.085741	56.906842
2666.385645	165603.142218	56.911847
2665.964025	165489.940952	56.916852
2664.805474	165379.997462	56.921857
2664.500540	165263.981043	56.926861
2663.667330	165147.362069	56.931866
2662.858341	165038.483150	56.936871
2662.541632	164932.807055	56.941876
2661.533851	164830.394097	56.946881
2660.953975	164710.443166	56.951885
2660.135563	164607.733810	56.956890
2659.809277	164496.554894	56.961895
2659.292016	164379.366986	56.966900
2658.356641	164269.289745	56.971905
2657.820967	164140.585841	56.976909
2657.321117	164039.582254	56.981914
2656.294894	163932.012526	56.986919
2655.824794	163820.985599	56.991924
2655.097601	163705.269884	56.996929
2654.484885	163586.942611	57.001933
2653.816796	163493.697700	57.006938
2652.802889	163371.264305	57.011943
2652.730711	163258.688444	57.016948
2651.502011	163168.241392	57.021953
2650.939028	163050.302141	57.026957
2650.339188	162941.281919	57.031962
2649.765200	162834.393945	57.036967
2649.258651	162714.183691	57.041972
2648.720067	162611.855215	57.046977
2647.926111	162482.854833	57.051981
2647.304096	162372.415849	57.056986
2646.944785	162258.146756	57.061991
2646.205840	162147.180283	57.066996
2645.099111	162037.213272	57.072001
2644.695035	161923.829609	57.077005
2644.235143	161809.298174	57.082010
2643.137110	161689.935197	57.087015
2642.518161	161579.269322	57.092020
2641.709290	161476.058799	57.097025
2641.572987	161354.917179	57.102029
2640.525703	161248.172500	57.107034
2639.694954	161141.838815	57.112039
2639.444401	161018.618668	57.117044
2638.570376	160919.679186	57.122049
2637.945788	160798.197279	57.127053
2637.367870	160679.212976	57.132058
2636.511921	160571.677201	57.137063
2635.825158	160464.331076	57.142068
2635.300603	160355.230539	57.147073
2635.058973	160231.020066	57.152077
2633.933357	160126.045643	57.157082
2633.261887	160012.443471	57.162087
2633.018838	159900.401088	57.167092
2632.011647	159790.577836	57.172097
2631.449217	159670.068889	57.177101
2630.761842	159563.068868	57.182106
2630.090483	159449.951600	57.187111
2629.505401	159345.008283	57.192116
2628.588111	159226.019104	57.197121
2628.040346	159109.590663	57.202125
2627.349199	159000.202910	57.207130
2626.572362	158896.155811	57.212135
2626.503549	158771.643437	57.217140
2625.722107	158667.699453	57.222145
2624.825285	158541.513876	57.227149
2624.253329	158429.235929	57.232154
2623.678864	158308.250506	57.237159
2622.968939	158196.071452	57.242164
2621.906605	158089.847284	57.247169
2621.551188	157964.175515	57.252173
2620.809319	157849.116882	57.257178
2619.799454	157746.000041	57.262183
2619.569302	157631.356838	57.267188
2618.637192	157524.300176	57.272193
2617.965111	157404.248684	57.277197
2617.756212	157294.319542	57.282202
2616.734521	157184.761082	57.287207
2616.476890	157065.471401	57.292212
2615.411197	156959.416514	57.297217
2614.961710	156841.810606	57.302221
2614.319181	156723.307703	57.307226
2613.589607	156617.213328	57.312231
2613.144593	156493.467950	57.317236
2612.325335	156379.392626	57.322241
2611.417560	156268.077502	57.327245
2610.672052	156156.126855	57.332250
2610.162741	156045.995088	57.337255
2609.716419	155929.256233	57.342260
2608.826526	155820.901606	57.347265
2608.480142	155708.507832	57.352269
2607.913600	155592.526469	57.357274
2606.810294	155482.897431	57.362279
2606.702943	155369.894875	57.367284
2605.652846	155258.478500	57.372289
2605.135021	155136.885155	57.377293
2604.582651	155018.221373	57.382298
2603.959956	154901.653837	57.387303
2603.552548	154774.781745	57.392308
2602.450630	154663.108611	57.397313
2602.257925	154536.826251	57.402317
2601.229666	154429.908977	57.407322
2600.258301	154308.733700	57.412327
2599.955472	154182.304878	57.417332
2599.063670	154071.947807	57.422337
2598.363710	153957.404160	57.427341
2597.642439	153840.754242	57.432346
2597.038808	153722.878541	57.437351
2596.611767	153614.533943	57.442356
2595.485911	153505.448803	57.447361
2595.147623	153385.231565	57.452365
2594.608078	153266.597379	57.457370
2593.846030	153149.219115	57.462375
2593.366079	153031.618612	57.467380
2592.303179	152918.508820	57.472385
2591.918021	152798.644321	57.477389
2591.144718	152693.967433	57.482394
2590.734827	152570.930017	57.487399
2590.132299	152455.816841	57.492404
2589.142566	152364.483250	57.497409
2588.754340	152167.977173	57.502413
2588.415875	152034.927317	57.507418
2587.437601	151923.752214	57.512423
2586.703830	151801.124887	57.517428
2586.095361	151678.783207	57.522433
2585.533033	151557.209993	57.527437
2584.893183	151448.652015	57.532442
2584.238159	151314.307967	57.537447
2583.432910	151196.193612	57.542452
2582.403176	151082.995909	57.547457
2582.244277	150962.466745	57.552461
2581.621827	150845.710078	57.557466
2581.038674	150729.455996	57.562471
2580.621017	150588.849474	57.567476
2579.906229	150480.052398	57.572481
2579.059074	150351.055461	57.577485
2578.118484	150232.927921	57.582490
2577.331421	150115.462802	57.587495
2576.844241	149995.789953	57.592500
2576.079564	149873.187487	57.597505
2575.722284	149750.571762	57.602509
2574.788444	149627.259888	57.607514
2574.138314	149504.348352	57.612519
2573.974260	149382.898086	57.617524
2572.674337	149268.961561	57.622529
2572.501910	149143.942205	57.627533
2571.614704	149035.685689	57.632538
2571.144284	148903.787968	57.637543
2570.646892	148777.741257	57.642548
2569.498629	148662.321304	57.647553
2569.032999	148526.306637	57.652557
2568.228130	148416.526792	57.657562
2567.640164	148288.907739	57.662567
2566.899249	148154.781074	57.667572
2566.130249	148052.583995	57.672577
2565.764481	147939.126896	57.677581
2564.815262	147805.466814	57.682586
2564.415818	147694.265370	57.687591
2563.921653	147574.005357	57.692596
2562.849297	147456.226647	57.697601
2562.372897	147324.692242	57.702605
2561.753390	147201.136578	57.707610
2560.904111	147073.678194	57.712615
2560.329409	146954.157678	57.717620
2559.655682	146836.483310	57.722625
2559.142497	146709.430631	57.727629
2558.536088	146595.444607	57.732634
2557.328055	146477.589384	57.737639
2556.969594	146349.979890	57.742644
2556.026726	146238.691777	57.747649
2555.615049	146109.808173	57.752653
2554.806880	145997.660836	57.757658
2553.974606	145877.651494	57.762663
2553.762240	145773.810494	57.767668
2553.013961	145661.604038	57.772673
2552.567855	145524.252149	57.777677
2551.756734	145406.604916	57.782682
2551.434402	145283.683204	57.787687
2550.889373	145154.290945	57.792692
2549.774152	145026.603458	57.797697
2549.081439	144912.154353	57.802701
2548.197412	144798.714468	57.807706
2547.493980	144669.883046	57.812711
2547.272534	144543.555374	57.817716
2546.284536	144432.611253	57.822721
2545.884762	144311.383031	57.827725
2545.068356	144185.557748	57.832730
2544.017613	144072.172362	57.837735
2543.905633	143950.061267	57.842740
2543.042098	143841.895120	57.847745
2542.665953	143709.267224	57.852749
2541.884204	143582.231737	57.857754
2541.222154	143457.655662	57.862759
2540.457658	143328.877632	57.867764
2539.653978	143230.717199	57.872769
2539.288942	143097.531078	57.877773
2538.510922	142977.384598	57.882778
2538.047697	142856.057800	57.887783
2537.699724	142733.912696	57.892788
2536.635100	142606.646537	57.897793
2536.047357	142475.811022	57.902797
2535.518633	142362.463579	57.907802
2535.008444	142235.416051	57.912807
2534.536401	142099.964072	57.917812
2533.654704	141978.783324	57.922817
2532.802824	141851.194357	57.927821
2532.360231	141728.026363	57.932826
2531.577677	141600.440169	57.937831
2531.221827	141457.755519	57.942836
2530.347702	141335.140350	57.947841
2529.465980	141206.542341	57.952845
2528.924623	141085.501814	57.957850
2528.194051	140955.457847	57.962855
2527.572333	140824.279072	57.967860
2526.822969	140708.342670	57.972865
2526.246760	140568.860893	57.977869
2525.144798	140443.934894	57.982874
2524.373402	140325.144677	57.987879
2524.024217	140204.280524	57.992884
2523.176837	140091.233506	57.997889
2522.626241	139969.233312	58.002893
2521.929638	139844.042276	58.007898
2521.333288	139737.614465	58.012903
2521.084029	139596.636972	58.017908
2520.113447	139480.257579	58.022913
2519.673661	139351.038439	58.027917
2518.591764	139226.431977	58.032922
2518.079834	139105.890278	58.037927
2517.754750	138976.044738	58.042932
2516.898001	138845.381976	58.047937
2516.200275	138732.570489	58.052941
2515.670563	138602.733604	58.057946
2514.798531	138482.747003	58.062951
2514.326259	138346.524289	58.067956
2513.364435	138242.586378	58.072961
2513.004951	138100.502724	58.077965
2512.071144	137978.507912	58.082970
2511.283544	137860.022312	58.087975
2510.782772	137732.001422	58.092980
2510.087208	137609.093764	58.097985
2509.760735	137477.641546	58.102989
2509.094393	137357.347423	58.107994
2508.294878	137234.445103	58.112999
2507.670547	137103.638874	58.118004
2506.683782	136990.066794	58.123009
2506.329290	136856.080955	58.128013
2505.888800	136731.764489	58.133018
2505.274153	136606.307382	58.138023
2504.712602	136473.537593	58.143028
2503.817067	136352.407351	58.148033
2503.271205	136215.875876	58.153037
2502.569795	136088.770537	58.158042
2502.012736	135969.214330	58.163047
2501.389091	135837.422769	58.168052
2500.457000	135704.842255	58.173057
2500.002126	135581.104643	58.178061
2499.600565	135447.844140	58.183066
2498.628060	135304.016512	58.188071
2498.207486	135193.321614	58.193076
2497.381033	135055.722169	58.198081
2496.962621	134908.632832	58.203085
2496.056527	134779.215567	58.208090
2495.533949	134659.964178	58.213095
2494.899074	134507.118536	58.218100
2493.910686	134391.791147	58.223105
2493.502552	134249.149632	58.228109
2492.930076	134107.398676	58.233114
2491.991444	134002.328968	58.238119
2491.051612	133858.465273	58.243124
2490.657163	133723.229971	58.248129
2490.057649	133606.218144	58.253133
2489.277670	133465.786233	58.258138
2488.576998	133343.316660	58.263143
2488.070862	133200.454552	58.268148
2487.428287	133081.838474	58.273153
2486.704796	132947.713311	58.278157
2486.414909	132812.186296	58.283162
2485.354816	132679.995706	58.288167
2484.705395	132555.527131	58.293172
2484.328247	132425.985863	58.298177
2483.472100	132288.531454	58.303181
2483.052314	132148.607846	58.308186
2482.190386	132021.177609	58.313191
2481.776556	131880.987637	58.318196
2480.939858	131760.337435	58.323201
2480.119377	131626.373621	58.328205
2479.968955	131488.912848	58.333210
2479.274996	131351.983466	58.338215
2478.529390	131200.201977	58.343220
2477.683632	131073.942014	58.348225
2477.168327	130941.927237	58.353229
2476.181738	130805.974116	58.358234
2475.154215	130673.940186	58.363239
2474.658647	130537.034136	58.368244
2474.081968	130425.544244	58.373249
2473.389624	130288.721407	58.378253
2473.096887	130155.697060	58.383258
2472.072790	130023.513245	58.388263
2471.567232	129886.142027	58.393268
2470.959680	129763.965368	58.398273
2470.297833	129614.706709	58.403277
2469.260064	129483.276985	58.408282
2468.828717	129367.831010	58.413287
2468.466462	129227.684246	58.418292
2467.662581	129104.944672	58.423297
2467.020082	128976.388558	58.428301
2466.235539	128842.483204	58.433306
2465.810867	128701.320248	58.438311
2465.326526	128563.088580	58.443316
2464.336952	128428.061995	58.448321
2463.627658	128294.515682	58.453325
2463.003640	128160.486588	58.458330
2462.235296	128031.446814	58.463335
2461.964393	127894.759491	58.468340
2461.237670	127769.524397	58.473345
2460.563276	127627.492123	58.478349
2460.077581	127497.597248	58.483354
2459.260702	127360.275239	58.488359
2458.915195	127222.295000	58.493364
2457.615825	127089.381488	58.498369
2457.075302	126941.984938	58.503373
2456.607151	126802.400698	58.508378
2456.058194	126662.791883	58.513383
2455.324017	126532.039317	58.518388
2454.510824	126405.427234	58.523393
2454.011477	126257.519879	58.528397
2453.324007	126117.872321	58.533402
2452.497398	125982.870075	58.538407
2452.083053	125843.637804	58.543412
2451.128758	125701.558343	58.548417
2450.813979	125570.794719	58.553421
2450.108533	125444.043054	58.558426
2449.204566	125299.456021	58.563431
2448.605937	125163.316914	58.568436
2447.920903	125026.900119	58.573441
2446.942204	124886.238389	58.578445
2446.674045	124762.950857	58.583450
2445.955762	124626.325485	58.588455
2445.439866	124480.436863	58.593460
2444.434951	124357.661644	58.598465
2443.880821	124217.863098	58.603469
2443.571714	124071.042330	58.608474
2442.836956	123938.791313	58.613479
2442.430575	123798.171540	58.618484
2441.599861	123662.635558	58.623489
2440.713010	123520.328371	58.628493
2440.240977	123385.486123	58.633498
2439.715538	123240.354960	58.638503
2439.000191	123085.604285	58.643508
2437.989820	122961.807822	58.648513
2437.570637	122826.871140	58.653517
2436.829837	122688.214908	58.658522
2435.954698	122551.332975	58.663527
2435.359360	122404.693741	58.668532
2434.643876	122274.555739	58.673537
2433.993231	122134.262832	58.678541
2433.219215	121999.119973	58.683546
2432.879790	121862.055098	58.688551
2432.080490	121722.752942	58.693556
2431.503929	121595.795968	58.698561
2430.992869	121455.179811	58.703565
2430.515587	121313.987682	58.708570
2429.476123	121176.288231	58.713575
2429.190642	121028.096584	58.718580
2428.002815	120910.318127	58.723585
2427.652967	120762.836510	58.728589
2426.902687	120619.279010	58.733594
2426.068932	120482.274307	58.738599
2425.382617	120336.137147	58.743604
2424.649963	120210.246398	58.748609
2424.124122	120065.215304	58.753613
2423.464983	119925.392621	58.758618
2423.095279	119788.032324	58.763623
2422.300242	119646.747213	58.768628
2421.443779	119507.345295	58.773633
2420.561596	119368.195778	58.778637
2420.156419	119240.873924	58.783642
2419.241448	119103.946483	58.788647
2418.735966	118955.592004	58.793652
2418.161148	118836.716420	58.798657
2417.478017	118688.328159	58.803661
2416.923927	118549.924508	58.808666
2416.004995	118409.668749	58.813671
2415.215171	118286.792570	58.818676
2414.789303	118166.493594	58.823681
2414.105063	118012.320240	58.828685
2413.521827	117874.381874	58.833690
2412.667324	117750.845654	58.838695
2412.215232	117612.208703	58.843700
2411.643174	117476.086123	58.848705
2410.908844	117331.008203	58.853709
2410.524692	117217.479898	58.858714
2409.712263	117050.840715	58.863719
2409.009127	116925.970545	58.868724
2408.532558	116780.099534	58.873729
2407.798539	116648.945325	58.878733
2407.578068	116481.048087	58.883738
2406.685499	116358.419604	58.888743
2405.746179	116212.955266	58.893748
2405.140899	116072.884732	58.898753
2404.558550	115905.569138	58.903757
2403.747678	115790.972344	58.908762
2402.893685	115659.277362	58.913767
2402.502407	115495.387023	58.918772
2401.707050	115384.781931	58.923777
2401.389643	115215.143943	58.928781
2400.529248	115099.422014	58.933786
2400.093113	114950.426031	58.938791
2399.329606	114799.083695	58.943796
2398.631061	114666.106205	58.948801
2398.202982	114519.904119	58.953805
2397.440421	114372.143823	58.958810
2396.727360	114221.209506	58.963815
2396.096345	114100.848040	58.968820
2395.285923	113922.582839	58.973825
2394.542606	113810.643606	58.978829
2393.719471	113657.902289	58.983834
2393.334189	113522.450427	58.988839
2392.707044	113356.910517	58.993844
2392.043474	113237.199367	58.998849
2391.339026	113110.736254	59.003853
2390.943408	112945.371797	59.008858
2389.889471	112822.640155	59.013863
2389.423486	112669.607095	59.018868
2388.926530	112526.657882	59.023873
2388.071761	112378.822449	59.028877
2387.681549	112225.894338	59.033882
2386.311935	112090.682487	59.038887
2386.171682	111949.323716	59.043892
2385.552953	111821.051255	59.048897
2384.500587	111666.664081	59.053901
2384.045955	111521.442040	59.058906
2383.162329	111376.796558	59.063911
2382.705704	111247.092549	59.068916
2381.983525	111103.248055	59.073921
2381.462240	110957.874904	59.078925
2380.993208	110818.256411	59.083930
2380.033292	110673.094101	59.088935
2379.799567	110525.387051	59.093940
2378.604042	110387.548806	59.098945
2378.276334	110217.400744	59.103949
2377.343268	110088.412969	59.108954
2376.890045	109963.582363	59.113959
2376.461057	109808.904952	59.118964
2375.222917	109656.387414	59.123969
2374.834491	109529.549884	59.128973
2374.333868	109373.528635	59.133978
2373.297324	109238.406591	59.138983
2372.900911	109096.210132	59.143988
2371.872088	108942.540727	59.148993
2371.210087	108801.904658	59.153997
2371.188325	108668.369856	59.159002
2370.307344	108522.363889	59.164007
2369.557715	108377.150169	59.169012
2368.665419	108232.074155	59.174017
2368.267650	108104.446043	59.179021
2367.832697	107952.617689	59.184026
2367.107632	107802.676375	59.189031
2366.392074	107650.202797	59.194036
2365.585930	107501.373912	59.199041
2364.926055	107368.188577	59.204045
2364.370235	107229.689427	59.209050
2363.706706	107072.706323	59.214055
2363.181234	106923.823815	59.219060
2362.189519	106782.737847	59.224065
2361.560651	106648.802890	59.229069
2360.893958	106506.004670	59.234074
2360.142159	106362.300810	59.239079
2359.771852	106211.843656	59.244084
2359.019314	106069.271030	59.249089
2358.029787	105921.178940	59.254093
2357.770781	105774.405809	59.259098
2356.892759	105630.942078	59.264103
2356.705971	105489.000143	59.269108
2355.574242	105354.746129	59.274113
2355.266797	105205.211648	59.279117
2354.700661	105055.573206	59.284122
2353.780920	104914.176000	59.289127
2353.444455	104754.929398	59.294132
2352.138299	104609.071788	59.299137
2351.587833	104469.426798	59.304141
2350.946277	104327.963602	59.309146
2350.570201	104180.679622	59.314151
2350.479527	104024.856524	59.319156
2348.981572	103881.863295	59.324161
2348.580902	103741.266276	59.329165
2348.046698	103584.501369	59.334170
2347.192434	103441.986047	59.339175
2346.310652	103294.978108	59.344180
2345.708216	103151.720437	59.349185
2345.060628	103001.968357	59.354189
2344.374665	102847.941250	59.359194
2343.550982	102724.678885	59.364199
2343.250815	102579.156459	59.369204
2342.548762	102442.034279	59.374209
2342.137758	102282.175500	59.379213
2341.461186	102135.795691	59.384218
2340.712243	101995.454670	59.389223
2340.154568	101838.730537	59.394228
2339.257710	101692.800770	59.399233
2338.976104	101542.898506	59.404237
2338.077891	101395.289806	59.409242
2337.342357	101245.277484	59.414247
2336.642712	101095.824996	59.419252
2336.142666	100957.309365	59.424257
2335.103872	100807.386024	59.429261
2334.726082	100650.305189	59.434266
2333.826946	100512.261471	59.439271
2333.249306	100354.009137	59.444276
2332.551333	100215.795742	59.449281
2331.837587	100067.779324	59.454285
2331.255135	99926.821831	59.459290
2330.260050	99785.017248	59.464295
2330.093793	99638.274164	59.469300
2329.296594	99485.650728	59.474305
2328.415799	99337.982638	59.479309
2327.882939	99181.209142	59.484314
2327.407980	99048.434888	59.489319
2326.501080	98904.141739	59.494324
2325.790327	98749.777926	59.499329
2325.375580	98616.914169	59.504333
2325.015580	98469.137377	59.509338
2323.900706	98323.542582	59.514343
2323.435513	98154.777942	59.519348
2322.815876	98033.404659	59.524353
2322.063185	97885.199207	59.529357
2321.570909	97725.651266	59.534362
2320.875147	97579.829859	59.539367
2320.303893	97430.108144	59.544372
2319.421526	97275.565887	59.549377
2318.669821	97153.362039	59.554381
2318.187427	96990.101145	59.559386
2317.750514	96848.429234	59.564391
2317.403155	96681.540463	59.569396
2316.185137	96536.309615	59.574401
2315.659345	96387.018843	59.579405
2315.135054	96235.458390	59.584410
2314.379712	96094.469559	59.589415
2313.829801	95931.810472	59.594420
2313.266919	95778.198097	59.599425
2312.489665	95626.117434	59.604429
2311.635368	95468.456580	59.609434
2310.791529	95338.020198	59.614439
2310.446848	95181.466444	59.619444
2309.957117	95031.253059	59.624449
2309.227453	94874.502494	59.629453
2308.503378	94716.154069	59.634458
2307.593356	94563.714833	59.639463
2307.090866	94406.018346	59.644468
2306.208827	94264.243062	59.649473
2305.669587	94119.801665	59.654477
2304.927770	93965.906684	59.659482
2304.195011	93817.014613	59.664487
2303.512131	93675.553922	59.669492
2303.096103	93505.452941	59.674497
2302.336742	93370.677271	59.679501
2301.891670	93228.363701	59.684506
2301.089836	93054.364155	59.689511
2300.139003	92913.927339	59.694516
2299.370646	92783.449550	59.699521
2298.839768	92617.032356	59.704525
2298.586033	92478.751469	59.709530
2297.166926	92332.730174	59.714535
2296.933141	92180.453688	59.719540
2296.393123	92044.750912	59.724545
2295.545823	91887.906925	59.729549
2295.096753	91736.720210	59.734554
2294.015516	91590.517100	59.739559
2293.649239	91442.438882	59.744564
2293.078022	91307.233831	59.749569
2292.569685	91152.262530	59.754573
2291.766050	90994.821983	59.759578
2290.966586	90844.172521	59.764583
2290.478797	90704.259690	59.769588
2289.767836	90578.642627	59.774593
2289.207068	90400.181237	59.779597
2288.167964	90268.220626	59.784602
2287.620766	90106.649987	59.789607
2286.992690	89950.945362	59.794612
2286.024167	89828.752786	59.799617
2286.006723	89675.685888	59.804621
2285.536804	89522.457245	59.809626
2284.449156	89373.626184	59.814631
2283.952042	89213.569496	59.819636
2283.095834	89051.022292	59.824641
2282.560123	88908.275633	59.829645
2281.890526	88757.499555	59.834650
2281.125073	88604.717337	59.839655
2280.927135	88467.448314	59.844660
2280.323452	88304.169296	59.849665
2279.031446	88144.348019	59.854669
2278.591263	87983.549661	59.859674
2277.697227	87846.559817	59.864679
2277.291755	87711.166995	59.869684
2276.638448	87561.962550	59.874689
2275.921379	87405.180944	59.879693
2275.409471	87255.746997	59.884698
2274.569874	87099.950641	59.889703
2274.191506	86941.603596	59.894708
2273.608523	86800.672420	59.899713
2272.753181	86640.678971	59.904718
2272.384985	86501.243450	59.909722
2271.743092	86330.422860	59.914727
2270.914438	86168.070562	59.919732
2270.151036	86017.911778	59.924737
2269.480368	85881.976706	59.929742
2268.908164	85699.796987	59.934746
2267.859600	85571.841162	59.939751
2267.620733	85403.677124	59.944756
2266.700958	85239.064377	59.949761
2265.787921	85116.034066	59.954766
2265.742085	84947.995148	59.959770
2264.591556	84792.410760	59.964775
2263.635275	84656.947180	59.969780
2263.187426	84497.260180	59.974785
2262.682280	84328.316547	59.979790
2261.734826	84200.714263	59.984794
2260.838747	84056.415475	59.989799
2260.669019	83915.152654	59.994804
2259.812713	83748.658934	59.999809
2259.283449	83611.917370	60.004814
2258.806205	83460.615783	60.009818
2258.222848	83310.396935	60.014823
2257.767172	83162.605445	60.019828
2257.079203	83008.082717	60.024833
2256.628870	82850.956512	60.029838
2255.758282	82699.912936	60.034842
2254.603520	82540.289522	60.039847
2254.179540	82380.678174	60.044852
2253.605567	82230.002909	60.049857
2252.749889	82081.978267	60.054862
2252.448406	81925.786077	60.059866
2251.946648	81774.247043	60.064871
2251.175802	81622.466594	60.069876
2250.617287	81460.247135	60.074881
2249.731510	81303.594569	60.079886
2249.270484	81152.738059	60.084890
2248.408722	80988.409270	60.089895
2248.272503	80817.622899	60.094900
2247.297245	80671.198952	60.099905
2246.396022	80519.276132	60.104910
2245.503098	80351.047181	60.109914
2244.869458	80206.017248	60.114919
2244.131085	80055.009925	60.119924
2243.529263	79896.713299	60.124929
2243.039131	79754.445796	60.129934
2242.310283	79600.252709	60.134938
2241.827639	79449.766916	60.139943
2241.403042	79279.945182	60.144948
2240.375632	79128.426500	60.149953
2239.796099	78971.318456	60.154958
2239.057715	78814.141758	60.159962
2238.420902	78653.395209	60.164967
2237.873660	78491.038851	60.169972
2237.132325	78352.698982	60.174977
2236.458097	78188.780985	60.179982
2236.016129	78033.464253	60.184986
2235.013955	77901.163243	60.189991
2234.690684	77730.045611	60.194996
2233.738544	77573.096108	60.200001
2233.061375	77417.409499	60.205006
2232.423628	77262.497200	60.210010
2231.712435	77112.844203	60.215015
2231.680231	76946.046369	60.220020
2230.373600	76792.371605	60.225025
2230.078664	76641.338116	60.230030
2229.384867	76477.202552	60.235034
2228.447200	76339.553779	60.240039
2228.111383	76163.781618	60.245044
2227.373354	76002.444766	60.250049
2226.484155	75855.623443	60.255054
2225.640168	75700.179218	60.260058
2225.155576	75547.150154	60.265063
2224.418467	75366.988148	60.270068
2223.448302	75237.480839	60.275073
2223.077803	75081.231331	60.280078
2222.524433	74918.302605	60.285082
2221.417905	74776.535102	60.290087
2221.015034	74637.539656	60.295092
2220.707945	74459.439968	60.300097
2219.800141	74318.436113	60.305102
2219.300525	74171.375213	60.310106
2218.458806	74013.200436	60.315111
2218.120369	73850.182930	60.320116
2217.419460	73698.811417	60.325121
2216.500393	73543.731552	60.330126
2216.208739	73383.428230	60.335130
2215.318826	73215.371909	60.340135
2214.732042	73069.460587	60.345140
2214.223972	72910.924859	60.350145
2213.290377	72756.695974	60.355150
2212.546013	72598.250899	60.360154
2211.419379	72450.301226	60.365159
2211.337806	72298.474681	60.370164
2210.388654	72152.887292	60.375169
2209.767929	71994.212041	60.380174
2209.310272	71840.396214	60.385178
2208.482220	71694.678957	60.390183
2207.934292	71531.105548	60.395188
2207.323815	71382.492856	60.400193
2206.528904	71232.105216	60.405198
2206.034075	71074.145835	60.410202
2205.481202	70923.696812	60.415207
2205.147311	70763.839414	60.420212
2204.200988	70604.067795	60.425217
2203.525474	70447.402617	60.430222
2202.754192	70289.936772	60.435226
2201.976521	70147.149341	60.440231
2201.405189	69989.160127	60.445236
2200.721619	69829.137769	60.450241
2200.008583	69674.486258	60.455246
2199.835984	69518.439114	60.460250
2198.780659	69365.516494	60.465255
2198.416335	69194.440427	60.470260
2197.762752	69043.882440	60.475265
2197.155758	68887.586216	60.480270
2196.566345	68726.481210	60.485274
2195.716076	68559.078980	60.490279
2195.094190	68396.683462	60.495284
2194.574428	68233.563746	60.500289
2193.536330	68072.072985	60.505294
2192.905280	67922.957776	60.510298
2191.957457	67755.641270	60.515303
2191.581304	67600.034432	60.520308
2190.609821	67444.890612	60.525313
2189.984980	67279.534613	60.530318
2189.600017	67140.405481	60.535322
2189.064267	66982.226002	60.540327
2188.479465	66816.072809	60.545332
2187.707136	66664.719305	60.550337
2186.942891	66504.866910	60.555342
2186.583378	66342.158834	60.560346
2185.530474	66177.649619	60.565351
2185.530574	66020.589915	60.570356
2184.691218	65864.215611	60.575361
2183.641226	65707.790504	60.580366
2183.517449	65530.819219	60.585370
2182.611460	65377.546596	60.590375
2181.674137	65212.533367	60.595380
2181.111618	65063.179249	60.600385
2180.571772	64890.076188	60.605390
2180.070566	64732.618951	60.610394
2178.947836	64582.356948	60.615399
2178.571488	64404.679420	60.620404
2177.842638	64258.001687	60.625409
2176.802500	64095.471300	60.630414
2176.377865	63935.485132	60.635418
2175.757721	63779.349537	60.640423
2175.162520	63612.858483	60.645428
2174.499929	63459.955218	60.650433
2173.938607	63305.729586	60.655438
2173.411768	63136.040598	60.660442
2172.277682	62974.408490	60.665447
2171.914434	62821.184282	60.670452
2171.294203	62660.233137	60.675457
2170.526208	62503.121594	60.680462
2170.061751	62337.434601	60.685466
2169.393390	62180.854442	60.690471
2168.432662	62022.175605	60.695476
2167.682729	61864.531500	60.700481
2167.232732	61693.162276	60.705486
2166.437802	61537.009580	60.710490
2165.537634	61378.867876	60.715495
2165.244020	61228.013424	60.720500
2164.334776	61074.288552	60.725505
2163.689518	60916.417357	60.730510
2163.103836	60757.423777	60.735514
2162.405489	60600.839359	60.740519
2161.916207	60434.175923	60.745524
2160.960005	60284.320501	60.750529
2160.430546	60129.922695	60.755534
2160.021569	59960.655103	60.760538
2159.070142	59806.083183	60.765543
2158.153401	59655.064863	60.770548
2157.761341	59496.332992	60.775553
2157.123961	59329.079341	60.780558
2156.631485	59182.254826	60.785562
2155.907558	59025.222380	60.790567
2155.533739	58863.175861	60.795572
2154.531161	58697.030342	60.800577
2154.070556	58545.565670	60.805582
2153.431779	58378.592988	60.810586
2152.760973	58215.279390	60.815591
2151.990159	58058.895570	60.820596
2151.500616	57903.300846	60.825601
2150.642367	57729.200056	60.830606
2150.056828	57578.203046	60.835610
2149.077369	57424.471957	60.840615
2148.776957	57262.807575	60.845620
2148.040751	57095.165651	60.850625
2147.093414	56945.769351	60.855630
2146.870113	56786.321808	60.860634
2146.065995	56626.863358	60.865639
2145.713945	56456.821172	60.870644
2144.960614	56297.708808	60.875649
2144.252932	56137.372162	60.880654
2144.104682	55966.435045	60.885658
2142.751084	55805.036012	60.890663
2142.361748	55642.270192	60.895668
2141.622187	55479.779743	60.900673
2140.885204	55309.651032	60.905678
2140.195129	55144.491135	60.910682
2139.431271	54985.182981	60.915687
2139.120340	54823.924645	60.920692
2138.451368	54667.939583	60.925697
2137.874239	54501.811911	60.930702
2137.064500	54336.637175	60.935706
2136.190548	54169.673594	60.940711
2135.849521	54006.667868	60.945716
2135.205226	53838.876633	60.950721
2134.381404	53677.621224	60.955726
2133.923952	53513.416978	60.960730
2133.095388	53354.997209	60.965735
2132.353905	53186.790761	60.970740
2131.732325	53013.282670	60.975745
2131.023131	52839.166806	60.980750
2130.361863	52679.688564	60.985754
2129.647296	52528.060813	60.990759
2128.855545	52362.521523	60.995764
2128.129543	52188.974635	61.000769
2127.377475	52045.583386	61.005774
2127.169183	51874.691087	61.010778
2126.145953	51723.400676	61.015783
2125.174424	51558.596534	61.020788
2124.638403	51400.087399	61.025793
2124.040201	51243.570112	61.030798
2123.760165	51074.215462	61.035802
2122.550138	50919.977961	61.040807
2122.035714	50755.561094	61.045812
2121.551622	50606.880608	61.050817
2120.814845	50455.343473	61.055822
2120.331641	50290.372273	61.060826
2119.629046	50125.067256	61.065831
2118.911795	49958.298166	61.070836
2118.389657	49808.712901	61.075841
2117.581353	49652.799667	61.080846
2117.102760	49478.996172	61.085850
2115.920346	49330.383343	61.090855
2115.410268	49163.794447	61.095860
2114.853141	49009.302208	61.100865
2114.212516	48856.083613	61.105870
2113.567423	48697.179222	61.110874
2112.737653	48543.313205	61.115879
2112.205934	48380.875969	61.120884
2111.678762	48220.900574	61.125889
2111.238723	48056.016003	61.130894
2110.614494	47897.928441	61.135898
2109.913331	47746.127220	61.140903
2109.460437	47568.333699	61.145908
2108.755303	47406.363128	61.150913
2107.651436	47245.415752	61.155918
2107.211829	47081.773841	61.160922
2106.427515	46920.168248	61.165927
2105.591705	46764.319613	61.170932
2105.153301	46605.723876	61.175937
2104.644521	46441.611787	61.180942
2103.951567	46283.663484	61.185946
2103.002303	46113.456537	61.190951
2102.604877	45941.386115	61.195956
2102.141908	45782.023640	61.200961
2101.275138	45624.539013	61.205966
2100.828937	45455.356152	61.210970
2099.968915	45292.025365	61.215975
2099.287752	45117.503125	61.220980
2098.352060	44970.406074	61.225985
2097.649452	44805.340655	61.230990
2097.512170	44628.526264	61.235994
2096.717200	44478.188261	61.240999
2095.849491	44309.731740	61.246004
2095.714651	44144.797547	61.251009
2094.661849	43988.287026	61.256014
2094.006898	43823.318238	61.261018
2093.498978	43664.842460	61.266023
2092.839372	43490.118072	61.271028
2092.019947	43332.652991	61.276033
2091.299988	43155.939720	61.281038
2091.013988	42995.154748	61.286042
2090.000541	42835.773785	61.291047
2089.439391	42661.418462	61.296052
2088.707155	42499.595772	61.301057
2088.016303	42341.733519	61.306062
2087.471707	42165.986014	61.311066
2086.778783	42010.653750	61.316071
2086.291096	41848.361984	61.321076
2085.532494	41694.127627	61.326081
2084.781888	41515.326874	61.331086
2084.247253	41338.217047	61.336090
2083.341889	41188.342578	61.341095
2082.803589	41018.044549	61.346100
2081.987276	40857.224562	61.351105
2081.254769	40687.169331	61.356110
2080.747612	40526.387184	61.361114
2079.748698	40361.945631	61.366119
2079.653869	40201.844152	61.371124
2078.660906	40048.333701	61.376129
2077.534420	39880.995478	61.381134
2077.569321	39718.686804	61.386138
2076.710056	39564.452835	61.391143
2076.276127	39394.285637	61.396148
2075.630179	39239.521208	61.401153
2074.645964	39080.285939	61.406158
2073.836553	38902.871889	61.411162
2073.085671	38745.169325	61.416167
2072.732954	38587.144211	61.421172
2071.768728	38427.559380	61.426177
2071.219265	38268.038274	61.431182
2070.950933	38106.743144	61.436186
2070.046150	37950.547232	61.441191
2069.310657	37775.796779	61.446196
2068.834292	37617.033695	61.451201
2068.003120	37458.955940	61.456206
2067.647102	37287.898114	61.461210
2066.711136	37137.259655	61.466215
2066.367010	36969.369220	61.471220
2065.538470	36802.971988	61.476225
2064.745135	36639.921699	61.481230
2064.155870	36475.365916	61.486234
2063.325939	36325.426003	61.491239
2062.745189	36163.552581	61.496244
2062.232849	36000.797402	61.501249
2061.317234	35838.077770	61.506254
2060.821795	35678.376623	61.511258
2060.319908	35519.107919	61.516263
2059.456462	35348.991183	61.521268
2058.736927	35189.410871	61.526273
2057.951075	35031.291883	61.531278
2057.807944	34865.332986	61.536282
2056.714927	34708.637622	61.541287
2056.252112	34546.250654	61.546292
2055.818505	34378.849208	61.551297
2055.097929	34221.505093	61.556302
2054.510581	34051.014837	61.561306
2053.559523	33879.816001	61.566311
2052.858182	33735.078273	61.571316
2052.466204	33547.597329	61.576321
2051.521548	33409.696402	61.581326
2051.088515	33234.605586	61.586330
2050.184358	33070.858694	61.591335
2049.684341	32906.967112	61.596340
2049.113733	32752.885825	61.601345
2048.544773	32580.742194	61.606350
2047.834185	32417.680568	61.611354
2046.840305	32262.877762	61.616359
2046.470381	32094.951999	61.621364
2046.112204	31931.651207	61.626369
2044.885439	31767.290550	61.631374
2044.634762	31592.445756	61.636378
2043.663973	31437.572775	61.641383
2042.933274	31276.387006	61.646388
2042.318811	31114.702447	61.651393
2041.543815	30949.033172	61.656398
2040.716092	30774.212817	61.661402
2040.042210	30629.719176	61.666407
2039.293662	30471.952276	61.671412
2038.912294	30314.561544	61.676417
2037.943937	30161.060615	61.681422
2037.629306	30004.684524	61.686426
2036.846261	29854.997976	61.691431
2036.376400	29690.350003	61.696436
2035.603585	29522.065802	61.701441
2034.999755	29368.620324	61.706446
2034.410936	29196.796553	61.711450
2033.390060	29042.601949	61.716455
2033.179415	28884.366889	61.721460
2032.371041	28738.859137	61.726465
2031.691772	28554.660992	61.731470
2031.028494	28392.319158	61.736474
2030.302152	28251.436358	61.741479
2029.321366	28078.898288	61.746484
2028.540183	27931.462959	61.751489
2027.798415	27768.523716	61.756494
2027.140337	27633.207260	61.761498
2027.004121	27461.848169	61.766503
2026.523412	27305.612848	61.771508
2025.997005	27132.695228	61.776513
2025.132085	27005.699983	61.781518
2024.538540	26821.196751	61.786522
2023.768092	26665.643104	61.791527
2022.939567	26503.452289	61.796532
2022.128927	26344.059350	61.801537
2021.390932	26194.149871	61.806542
2021.133167	26025.167875	61.811546
2019.920784	25889.860037	61.816551
2019.456620	25726.663584	61.821556
2018.741425	25575.233567	61.826561
2017.976272	25421.680548	61.831566
2017.560818	25266.255479	61.836570
2016.901397	25114.390545	61.841575
2016.262357	24950.951749	61.846580
2015.489051	24803.551709	61.851585
2015.011615	24636.836773	61.856590
2014.523243	24487.939745	61.861594
2013.415027	24336.857854	61.866599
2012.818311	24171.581865	61.871604
2012.377855	24012.358691	61.876609
2011.600989	23869.772335	61.881614
2011.167324	23705.248403	61.886618
2010.131418	23555.472522	61.891623
2009.365856	23393.914425	61.896628
2008.648598	23255.673577	61.901633
2007.939296	23107.875544	61.906638
2007.346225	22962.648884	61.911642
2006.633338	22817.182780	61.916647
2006.140224	22642.534851	61.921652
2005.441837	22517.443925	61.926657
2004.329434	22367.236579	61.931662
2003.953399	22203.219675	61.936666
2003.152371	22072.431826	61.941671
2002.592827	21916.287727	61.946676
2001.975165	21767.901775	61.951681
2001.008065	21622.941796	61.956686
2000.571982	21472.733514	61.961690
1999.834721	21353.060195	61.966695
1999.018392	21195.697525	61.971700
1998.387041	21040.692284	61.976705
1997.592932	20924.380500	61.981710
1997.171611	20746.224736	61.986714
1996.002471	20637.907808	61.991719
1995.525560	20494.191029	61.996724
1994.475211	20351.574393	62.001729
1993.816126	20228.671279	62.006734
1993.363760	20089.486857	62.011738
1992.551546	19973.891587	62.016743
1991.642815	19815.933307	62.021748
1991.082713	19716.749623	62.026753
1989.892666	19552.433609	62.031758
1989.387637	19458.830695	62.036762
1988.356427	19339.584906	62.041767
1987.555781	19209.004370	62.046772
1986.563650	19117.715366	62.051777
1985.997127	18985.971015	62.056782
1985.152308	18888.733231	62.061786
1984.149917	18801.191222	62.066791
1983.559292	18692.913170	62.071796
1982.965824	18592.058075	62.076801
1982.316992	18495.423174	62.081806
1981.594922	18397.722949	62.086810
1980.475680	18308.638038	62.091815
1979.812038	18217.657404	62.096820
1978.881506	18119.023422	62.101825
1977.991619	18039.729296	62.106830
1977.557665	17963.619440	62.111834
1976.814003	17869.424149	62.116839
1975.810335	17791.388294	62.121844
1975.199062	17721.927133	62.126849
1974.695925	17624.309112	62.131854
1974.143809	17572.276896	62.136858
1973.462025	17488.919264	62.141863
1972.977868	17395.542713	62.146868
1972.084964	17328.974851	62.151873
1971.310309	17243.201861	62.156878
1970.992116	17158.531442	62.161882
1970.197842	17082.578616	62.166887
1969.188378	17016.517825	62.171892
1968.662517	16937.187937	62.176897
1968.277453	16859.249016	62.181902
1967.762243	16769.388973	62.186906
1966.595828	16707.779204	62.191911
1965.997200	16632.296982	62.196916
1965.459416	16556.740943	62.201921
1964.699032	16496.706588	62.206926
1964.193870	16415.917631	62.211930
1963.598434	16343.086036	62.216935
1962.654449	16268.133212	62.221940
1961.910432	16195.773039	62.226945
1961.249238	16127.998505	62.231950
1960.638560	16045.921554	62.236954
1959.604439	15998.042723	62.241959
1959.174521	15932.099207	62.246964
1958.609202	15864.702691	62.251969
1957.937334	15793.212219	62.256974
1957.288150	15729.674585	62.261978
1956.703554	15659.761372	62.266983
1955.960465	15596.006460	62.271988
1955.169859	15540.157155	62.276993
1954.526146	15461.506290	62.281998
1954.222284	15395.019613	62.287002
1953.352364	15331.790071	62.292007
1952.612673	15269.760697	62.297012
1951.918746	15204.983835	62.302017
1951.037951	15144.565140	62.307022
1950.548345	15076.385317	62.312026
1949.646854	15017.467308	62.317031
1949.390643	14955.341739	62.322036
1948.743330	14896.503710	62.327041
1947.944902	14835.771868	62.332046
1947.303547	14771.029337	62.337050
1946.684779	14711.893894	62.342055
1946.192682	14648.137311	62.347060
1945.465749	14580.533175	62.352065
1944.754697	14525.583625	62.357070
1944.490205	14451.132399	62.362074
1943.743321	14396.347238	62.367079
1942.780351	14339.805869	62.372084
1942.418866	14265.470186	62.377089
1941.203495	14201.226739	62.382094
1940.896895	14124.008573	62.387098
1939.842555	14086.469985	62.392103
1939.398218	14019.459138	62.397108
1939.202288	13953.766155	62.402113
1937.851489	13898.764357	62.407118
1937.654485	13840.302921	62.412122
1936.930490	13778.277275	62.417127
1936.515887	13707.918051	62.422132
1935.979837	13642.376285	62.427137
1934.871703	13576.896715	62.432142
1934.495065	13506.891461	62.437146
1933.689618	13443.242227	62.442151
1933.457985	13372.552465	62.447156
1932.574709	13311.729771	62.452161
1931.690261	13257.670518	62.457166
1931.314235	13183.641100	62.462170
1930.241164	13131.671318	62.467175
1929.525899	13066.436284	62.472180
1928.880793	13005.032107	62.477185
1928.170154	12942.755738	62.482190
1927.826662	12882.911833	62.487194
1927.131411	12830.926108	62.492199
1926.383741	12761.933783	62.497204
1925.886924	12696.740624	62.502209
1925.177957	12646.888727	62.507214
1924.732898	12571.720738	62.512218
1923.946836	12514.879903	62.517223
1923.184112	12440.727089	62.522228
1922.443934	12382.815551	62.527233
1921.718981	12312.418437	62.532238
1921.381889	12250.371457	62.537242
1920.457378	12198.649780	62.542247
1919.992697	12137.684848	62.547252
1919.364600	12071.737367	62.552257
1918.605099	12008.919633	62.557262
1917.856477	11948.911142	62.562266
1917.001463	11890.223929	62.567271
1916.312969	11824.357538	62.572276
1915.934360	11772.358908	62.577281
1914.889248	11723.012202	62.582286
1914.828483	11644.822865	62.587290
1914.077663	11600.622288	62.592295
1913.384162	11527.434884	62.597300
1912.939854	11462.393153	62.602305
1911.874106	11408.267887	62.607310
1911.219931	11341.457796	62.612314
1910.367762	11284.125904	62.617319
1909.818737	11227.218346	62.622324
1909.126161	11161.375810	62.627329
1908.438354	11106.974638	62.632334
1908.061355	11046.975430	62.637338
1907.181618	10996.609480	62.642343
1906.505414	10937.086261	62.647348
1906.197927	10870.061267	62.652353
1905.106706	10812.315432	62.657358
1904.604591	10754.036807	62.662362
1903.816989	10689.764206	62.667367
1903.451482	10632.279812	62.672372
1902.737174	10563.338964	62.677377
1902.055546	10515.180804	62.682382
1901.513828	10444.145114	62.687386
1900.911199	10379.562007	62.692391
1900.213009	10326.654539	62.697396
1899.725542	10267.982942	62.702401
1898.801884	10192.189509	62.707406
1898.004836	10142.283529	62.712410
1897.656914	10087.417466	62.717415
1896.995736	10020.756752	62.722420
1896.084083	9957.283333	62.727425
1894.993068	9908.684800	62.732430
1894.934232	9843.149788	62.737434
1894.135232	9792.505620	62.742439
1893.309794	9732.789158	62.747444
1893.052819	9668.279279	62.752449
1891.930829	9601.963411	62.757454
1891.612483	9539.632677	62.762458
1890.962316	9485.570250	62.767463
1890.176825	9421.338242	62.772468
1889.422014	9367.851825	62.777473
1888.392054	9322.617855	62.782478
1887.964367	9254.300221	62.787482
1887.149848	9201.734710	62.792487
1886.423361	9135.216107	62.797492
1886.023184	9097.998206	62.802497
1885.544218	9036.483603	62.807502
1884.554139	8963.212566	62.812506
1883.685466	8940.486275	62.817511
1883.063375	8866.958870	62.822516
1882.762116	8803.031315	62.827521
1882.033050	8772.176993	62.832526
1881.639891	8700.091305	62.837530
1880.954795	8639.322659	62.842535
1880.287678	8579.927257	62.847540
1879.896499	8526.618053	62.852545
1878.973588	8471.680761	62.857550
1878.479474	8395.221160	62.862554
1877.677769	8345.099838	62.867559
1877.071839	8272.630696	62.872564
1876.367223	8227.791746	62.877569
1875.667439	8175.016776	62.882574
1875.243503	8112.900443	62.887578
1874.775393	8057.391133	62.892583
1873.918516	7990.148501	62.897588
1873.366596	7931.648933	62.902593
1872.361165	7863.748084	62.907598
1871.874680	7793.183987	62.912602
1871.120849	7740.242433	62.917607
1870.334822	7675.765974	62.922612
1869.562215	7607.131979	62.927617
1868.778936	7560.893506	62.932622
1868.463929	7496.707486	62.937626
1867.635861	7441.227647	62.942631
1867.032412	7386.218789	62.947636
1866.412785	7334.582626	62.952641
1865.652437	7271.664166	62.957646
1865.180539	7202.671123	62.962650
1864.333090	7161.041008	62.967655
1863.752084	7099.414516	62.972660
1863.030675	7054.013026	62.977665
1862.297040	6986.096696	62.982670
1862.151628	6929.268775	62.987674
1861.359784	6860.631026	62.992679
1860.482635	6802.475454	62.997684
1859.514863	6744.205924	63.002689
1858.829230	6690.028321	63.007694
1858.510746	6617.470322	63.012698
1857.843596	6576.961715	63.017703
1856.859422	6517.457266	63.022708
1856.561211	6463.936779	63.027713
1855.434713	6411.775359	63.032718
1855.066987	6352.278603	63.037722
1853.925886	6304.228677	63.042727
1853.289367	6256.518422	63.047732
1853.021114	6201.149954	63.052737
1852.315153	6152.952550	63.057742
1851.732008	6093.407427	63.062746
1850.643061	6040.999202	63.067751
1850.273321	5983.953378	63.072756
1850.159348	5924.284747	63.077761
1849.218107	5874.436864	63.082766
1848.783084	5809.362228	63.087770
1848.011739	5762.644359	63.092775
1847.393072	5689.797033	63.097780
1846.648294	5631.442056	63.102785
1845.625246	5583.712529	63.107790
1845.201381	5516.673430	63.112794
1844.270080	5470.471694	63.117799
1843.728892	5415.187363	63.122804
1843.138608	5356.571532	63.127809
1842.347040	5315.054477	63.132814
1841.735147	5239.446945	63.137818
1840.754791	5204.188769	63.142823
1840.823645	5144.834192	63.147828
1839.940255	5083.291712	63.152833
1839.175444	5037.325177	63.157838
1838.685289	4976.252300	63.162842
1837.886134	4930.106994	63.167847
1837.060771	4867.719378	63.172852
1836.230212	4806.994654	63.177857
1835.911026	4751.137298	63.182862
1835.224158	4709.594285	63.187866
1834.442988	4651.774240	63.192871
1833.869530	4594.465639	63.197876
1833.276850	4554.472089	63.202881
1832.403795	4497.244565	63.207886
1832.065408	4426.351202	63.212890
1831.343857	4380.813628	63.217895
1830.714639	4324.078843	63.222900
1830.322994	4258.659505	63.227905
1829.234820	4202.244924	63.232910
1828.711226	4143.404081	63.237914
1827.988571	4088.998209	63.242919
1827.045537	4043.354892	63.247924
1826.845077	3979.236128	63.252929
1825.749027	3941.015070	63.257934
1825.530000	3867.730794	63.262938
1824.795300	3830.980268	63.267943
1824.004645	3785.763090	63.272948
1823.681859	3717.380943	63.277953
1822.561610	3661.156505	63.282958
1821.902633	3601.086179	63.287962
1821.128220	3546.207104	63.292967
1820.370991	3492.030545	63.297972
1820.209016	3439.247024	63.302977
1819.208205	3392.333385	63.307982
1818.708575	3337.655933	63.312986
1818.525495	3280.175333	63.317991
1817.576653	3226.650830	63.322996
1816.800888	3170.130684	63.328001
1816.046752	3109.441859	63.333006
1815.400171	3048.669964	63.338010
1814.267936	3006.984845	63.343015
1813.602099	2972.294065	63.348020
1813.128109	2903.045448	63.353025
1812.429363	2868.495781	63.358030
1812.163346	2817.961184	63.363034
1811.658739	2770.245238	63.368039
1810.744120	2712.810481	63.373044
1810.041748	2663.881100	63.378049
1809.409145	2603.111993	63.383054
1809.182980	2548.773374	63.388058
1807.855010	2492.309632	63.393063
1807.185288	2444.285826	63.398068
1806.928983	2372.836560	63.403073
1805.793544	2331.145213	63.408078
1805.508320	2289.222764	63.413082
1804.813219	2236.779005	63.418087
1804.075545	2179.849744	63.423092
1803.565650	2126.520590	63.428097
1802.755536	2087.985357	63.433102
1802.459941	2028.840814	63.438106
1801.355728	1974.083895	63.443111
1800.790340	1915.965190	63.448116
1800.391101	1863.443461	63.453121
1799.291820	1831.698486	63.458126
1798.656880	1754.039502	63.463130
1798.047674	1704.524491	63.468135
1797.194686	1653.928641	63.473140
1796.776048	1612.169686	63.478145
1795.600670	1551.566859	63.483150
1795.336413	1517.691043	63.488154
1794.625099	1474.357748	63.493159
1794.058524	1407.517801	63.498164
1793.589320	1364.075420	63.503169
1792.668650	1324.082874	63.508174
1792.184115	1265.341251	63.513178
1791.342614	1217.910196	63.518183
1790.396083	1164.916482	63.523188
1789.996174	1133.972703	63.528193
1789.115696	1080.979846	63.533198
1788.747221	1037.218084	63.538202
1787.784718	991.052033	63.543207
1787.393920	945.070524	63.548212
1786.657849	893.323324	63.553217
1785.610981	841.379657	63.558222
1785.388745	799.804741	63.563226
1784.801525	754.364394	63.568231
1784.048092	696.005252	63.573236
1783.376341	663.673761	63.578241
1782.546795	624.939711	63.583246
1782.062241	575.609031	63.588250
1781.306559	526.275845	63.593255
1780.294581	478.710283	63.598260
1779.745923	428.325848	63.603265
1778.472844	409.715182	63.608270
1778.046705	365.122522	63.613274
1777.627016	331.266276	63.618279
1776.823566	299.036941	63.623284
1776.074028	263.435545	63.628289
1775.515932	213.706202	63.633294
1774.955882	172.533656	63.638298
1774.623722	155.845952	63.643303
1773.707685	112.765284	63.648308
1772.841197	58.629120	63.653313
1771.940521	31.444556	63.658318
1771.411830	-5.637263	63.663322
1770.335820	-32.505289	63.668327
1769.351021	-59.600630	63.673332
1768.533707	-76.963188	63.678337
1765.255716	-16.881971	63.683342
1762.590064	30.854493	63.688346
1763.026016	32.944047	63.693351
1763.621508	35.659522	63.698356
1764.438939	25.863352	63.703361
1763.511380	41.357035	63.708366
1762.786526	22.530507	63.713370
1763.008871	23.271048	63.718375
1762.425344	41.985303	63.723380
1760.991417	29.331396	63.728385
1759.810958	33.456405	63.733390
1759.268383	37.366569	63.738394
1758.917611	43.345122	63.743399
1758.489815	39.264271	63.748404
1758.099132	42.956356	63.753409
1756.760509	50.014287	63.758414
1756.483058	38.737832	63.763418
1755.492521	37.884380	63.768423
1754.435968	49.453167	63.773428
1754.490931	35.350158	63.778433
1753.953508	53.855264	63.783438
1753.754681	41.520837	63.788442
1752.893266	48.242790	63.793447
1751.406303	45.881824	63.798452
1750.741642	42.822577	63.803457
1750.247782	48.158408	63.808462
1749.665183	42.555208	63.813466
1749.237538	48.230594	63.818471
1748.585558	45.233985	63.823476
1748.264758	37.529782	63.828481
1747.099819	46.882898	63.833486
1746.493483	48.060971	63.838490
1745.913422	44.228224	63.843495
1745.025378	49.120479	63.848500
1744.740629	50.179670	63.853505
1744.047433	54.366067	63.858510
1743.430939	43.618106	63.863514
1742.832943	48.339719	63.868519
1741.921613	45.050002	63.873524
1741.411926	36.513238	63.878529
1740.718511	53.483569	63.883534
1740.490178	33.072241	63.888538
1739.498050	37.906910	63.893543
1738.672883	34.575128	63.898548
1738.111844	55.400445	63.903553
1737.439293	42.024818	63.908558
1737.083487	40.800912	63.913562
1735.994616	41.901091	63.918567
1735.357149	49.316006	63.923572
1735.000047	35.153873	63.928577
1734.253234	50.445404	63.933582
1733.935252	37.278386	63.938586
1733.207165	49.056772	63.943591
1732.483975	40.997027	63.948596
1731.751590	36.311725	63.953601
1731.064579	48.619732	63.958606
1730.705477	50.550143	63.963610
1729.467891	47.184521	63.968615
1728.381971	40.797132	63.973620
1728.301499	38.055098	63.978625
1727.957825	46.440446	63.983630
1726.939506	35.802049	63.988634
1725.883402	46.393095	63.993639
1725.511650	40.176116	63.998644
1725.447615	33.653230	64.003649
1724.182512	37.883158	64.008654
1723.225065	39.422921	64.013658
1723.093173	43.774047	64.018663
1722.333733	45.988811	64.023668
1721.725957	40.813804	64.028673
1721.169705	41.443052	64.033678
1720.512561	45.226348	64.038682
1720.176984	46.342499	64.043687
1719.671524	47.674860	64.048692
1719.069258	43.487692	64.053697
1717.364936	41.763646	64.058702
1716.471370	44.113251	64.063706
1716.764385	42.649102	64.068711
1716.010900	53.286702	64.073716
1715.059083	46.381294	64.078721
1714.115275	47.849511	64.083726
1713.568023	46.069411	64.088730
1712.879103	46.494238	64.093735
1712.737969	38.772541	64.098740
1712.080597	38.613636	64.103745
1711.192755	42.280618	64.108750
1710.673391	40.502397	64.113754
1710.332177	52.058496	64.118759
1709.403672	60.825319	64.123764
1709.225367	44.206363	64.128769
1707.765331	53.305183	64.133774
1706.887635	52.821742	64.138778
1706.374203	46.428580	64.143783
1705.365209	48.610450	64.148788
1705.755490	48.816552	64.153793
1705.143973	54.388691	64.158798
1704.254705	52.828492	64.163802
1703.391766	53.001852	64.168807
1702.781185	51.581883	64.173812
1702.425102	46.564013	64.178817
1700.801828	54.646437	64.183822
1700.463336	42.859312	64.188826
1700.150929	51.178199	64.193831
1699.191403	51.147713	64.198836
1698.721499	47.169752	64.203841
1698.020480	62.931825	64.208846
1697.667820	53.986935	64.213850
1697.422440	47.095474	64.218855
1696.700001	53.085765	64.223860
1695.542042	48.160576	64.228865
1694.519450	48.083342	64.233870
1693.910369	43.206583	64.238874
1693.617120	48.606746	64.243879
1692.612589	55.345143	64.248884
1692.606173	49.120596	64.253889
1691.611658	47.525083	64.258894
1691.178225	45.466720	64.263898
1689.716902	45.620022	64.268903
1688.915874	53.981834	64.273908
1688.650426	50.813460	64.278913
1687.847866	52.809587	64.283918
1687.522404	46.172114	64.288922
1687.137023	45.233600	64.293927
1686.411260	53.234963	64.298932
1685.930901	48.394526	64.303937
1685.149491	45.696029	64.308942
1684.366482	42.321298	64.313946
1683.294944	51.937136	64.318951
1682.734352	51.920555	64.323956
1681.933275	50.478814	64.328961
1681.218928	48.676380	64.333966
1680.616487	47.491660	64.338970
1680.246354	43.974077	64.343975
1679.732579	56.259309	64.348980
1679.498460	44.774141	64.353985
1678.587354	51.087707	64.358990
1678.423472	46.834066	64.363994
1677.236024	41.484658	64.368999
1676.132557	46.773837	64.374004
1676.030208	42.447347	64.379009
1675.030977	48.798565	64.384014
1674.729043	50.650518	64.389018
1673.366531	51.013628	64.394023
1672.446486	48.573691	64.399028
1672.378423	52.540956	64.404033
1671.774703	44.657788	64.409038
1671.388032	51.949299	64.414042
1670.728721	46.949643	64.419047
1670.391523	56.291146	64.424052
1669.405417	47.163050	64.429057
1668.175544	46.596801	64.434062
1667.596941	42.910495	64.439066
1667.225264	44.890217	64.444071
1666.338767	52.537085	64.449076
1666.056046	42.693306	64.454081
1664.732650	57.814682	64.459086
1664.010112	45.580811	64.464090
1663.796833	45.408139	64.469095
1663.192014	58.496285	64.474100
1662.605814	38.408319	64.479105
1661.840838	48.265611	64.484110
1661.378178	52.752860	64.489114
1661.323046	48.932936	64.494119
1659.937029	56.545624	64.499124
1659.056330	44.300612	64.504129
1658.285326	54.627204	64.509134
1657.985862	42.234670	64.514138
1657.650995	47.469565	64.519143
1657.090932	54.257209	64.524148
1656.366971	49.827624	64.529153
1655.143370	55.454431	64.534158
1654.598261	57.606782	64.539162
1654.413657	40.708157	64.544167
1653.122372	57.016567	64.549172
1652.439474	40.695401	64.554177
1651.437383	61.568715	64.559182
1651.114593	46.666311	64.564186
1650.534833	42.978616	64.569191
1650.237527	51.556870	64.574196
1649.854382	29.380393	64.579201
1648.612317	58.723477	64.584206
1647.642210	50.423872	64.589210
1647.035314	35.717996	64.594215
1646.775474	64.532906	64.599220
1646.274366	37.319628	64.604225
1645.762278	43.509889	64.609230
1645.192105	51.407697	64.614234
1644.019325	54.065026	64.619239
1643.080300	53.979266	64.624244
1642.781176	38.637890	64.629249
1641.955428	48.848603	64.634254
1641.651445	43.978581	64.639258
1641.127778	44.765089	64.644263
1640.222370	52.755578	64.649268
1639.514864	51.466137	64.654273
1639.024577	50.116958	64.659278
1638.450861	39.832155	64.664282
1637.255657	52.337602	64.669287
1636.012343	52.697564	64.674292
1635.625751	45.738665	64.679297
1635.560632	52.100764	64.684302
1634.883235	47.444601	64.689306
1634.342825	43.838965	64.694311
1633.821304	45.762075	64.699316
1633.463835	50.562186	64.704321
1632.434897	53.337011	64.709326
1631.541153	43.118820	64.714330
1631.001633	46.875564	64.719335
1630.448915	50.766866	64.724340
1629.620318	49.261708	64.729345
1628.628302	43.939621	64.734350
1628.020532	55.517571	64.739354
1627.467646	36.711077	64.744359
1627.005654	48.426705	64.749364
1626.851354	43.408331	64.754369
1625.750250	46.338120	64.759374
1624.840983	52.876906	64.764378
1624.136450	53.408311	64.769383
1623.490496	51.479914	64.774388
1623.424094	41.169710	64.779393
1622.029516	54.872163	64.784398
1621.043052	46.185679	64.789402
1620.751799	43.824054	64.794407
1620.121662	45.888997	64.799412
1619.880465	42.180637	64.804417
1619.153247	47.324909	64.809422
1618.749007	45.451150	64.814426
1618.358433	53.911765	64.819431
1616.958931	51.560637	64.824436
1616.262878	46.133189	64.829441
1615.888823	51.300199	64.834446
1615.061290	44.589549	64.839450
1614.089547	41.609090	64.844455
1613.374508	45.726447	64.849460
1613.111749	35.598826	64.854465
1612.591960	47.432442	64.859470
1612.176427	44.696340	64.864474
1611.545616	49.082581	64.869479
1610.119753	58.843046	64.874484
1609.699824	53.467918	64.879489
1609.057924	44.878079	64.884494
1608.588718	42.785993	64.889498
1608.194931	44.363974	64.894503
1606.583808	44.999997	64.899508
1606.230083	32.437916	64.904513
1605.669092	42.805257	64.909518
1605.576869	41.837526	64.914522
1605.111610	37.508780	64.919527
1603.645224	46.696958	64.924532
1603.024478	43.960347	64.929537
1602.323011	46.840843	64.934542
1601.951336	42.872528	64.939546
1601.544667	42.271712	64.944551
1600.585426	43.457002	64.949556
1599.939156	33.483355	64.954561
1599.259051	43.745047	64.959566
1598.941124	44.006885	64.964570
1597.910553	43.434235	64.969575
1596.558386	44.774992	64.974580
1596.178280	36.227144	64.979585
1595.246973	39.210387	64.984590
1595.339699	44.153429	64.989594
1594.540919	47.440457	64.994599
1593.773735	44.446428	64.999604
1593.572501	36.737452	65.004609
1593.009726	48.021256	65.009614
1592.158113	42.005122	65.014618
1591.422213	38.178255	65.019623
1590.561081	46.600095	65.024628
1590.507962	42.257906	65.029633
1589.083232	48.763485	65.034638
1588.024286	33.575969	65.039642
1587.831967	35.336398	65.044647
1586.961922	54.192385	65.049652
1586.815457	41.714061	65.054657
1586.267369	40.716263	65.059662
1585.617034	41.347873	65.064666
1584.656664	36.340889	65.069671
1583.822963	45.463242	65.074676
1583.506390	38.762882	65.079681
1582.733923	44.485186	65.084686
1582.640484	39.797758	65.089690
1581.569555	34.773651	65.094695
1580.483195	31.420350	65.099700
1580.008831	39.772851	65.104705
1579.364701	44.079214	65.109710
1579.073605	40.370904	65.114714
1578.291303	31.864891	65.119719
1576.885874	44.690747	65.124724
1576.845000	42.283039	65.129729
1576.159910	45.993538	65.134734
1575.850224	40.053724	65.139738
1574.607525	35.347061	65.144743
1573.565326	42.736424	65.149748
1573.636363	38.320895	65.154753
1572.918853	34.705571	65.159758
1572.858051	44.496720	65.164762
1571.758389	39.682178	65.169767
1570.711406	48.767464	65.174772
1570.674388	43.001937	65.179777
1569.602917	43.902308	65.184782
1568.817337	43.546199	65.189786
1568.196893	44.931549	65.194791
1567.380105	49.055623	65.199796
1567.222671	30.271482	65.204801
1566.185577	43.661688	65.209806
1564.923349	41.370778	65.214810
1564.605146	32.240691	65.219815
1564.048538	43.042562	65.224820
1563.856437	34.594155	65.229825
1563.287762	39.484596	65.234830
1562.680165	40.677102	65.239834
1561.859154	38.218319	65.244839
1560.890498	52.840252	65.249844
1560.537912	51.764088	65.254849
1559.282799	45.596044	65.259854
1558.460676	42.990788	65.264858
1557.985982	48.232138	65.269863
1557.245734	51.268613	65.274868
1557.176224	46.962144	65.279873
1556.529619	47.110639	65.284878
1556.071333	47.356938	65.289882
1555.326245	42.850324	65.294887
1554.092565	43.990933	65.299892
1553.856484	42.013198	65.304897
1553.262892	49.971507	65.309902
1552.365591	52.742790	65.314906
1551.267660	43.069571	65.319911
1550.799883	47.174461	65.324916
1550.462062	34.934706	65.329921
1550.045588	52.520186	65.334926
1549.499024	34.540593	65.339930
1548.327036	35.975741	65.344935
1547.366442	44.728773	65.349940
1547.499281	26.693272	65.354945
1546.728559	44.342916	65.359950
1546.102618	44.899699	65.364954
1544.816107	46.794577	65.369959
1544.320161	52.663758	65.374964
1544.024869	40.535510	65.379969
1543.202719	43.692229	65.384974
1542.314445	44.672306	65.389978
1541.951840	37.132478	65.394983
1541.354743	47.995980	65.399988
1540.904902	48.551588	65.404993
1539.718417	47.864970	65.409998
1538.885384	42.732117	65.415002
1538.421831	38.639649	65.420007
1537.816050	50.895353	65.425012
1537.565870	54.191414	65.430017
1536.265342	47.043463	65.435022
1535.810113	48.963942	65.440026
1535.228588	40.615263	65.445031
1534.626076	50.419956	65.450036
1534.146814	35.408426	65.455041
1532.991288	48.077902	65.460046
1532.519597	39.595081	65.465050
1532.164021	40.676585	65.470055
1531.527850	48.767814	65.475060
1530.755121	42.294484	65.480065
1529.932256	39.208404	65.485070
1529.156504	48.495021	65.490074
1528.922760	48.625223	65.495079
1527.581813	53.832352	65.500084
1526.941013	44.154310	65.505089
1526.162408	46.003179	65.510094
1525.651609	48.422903	65.515098
1525.613414	41.358207	65.520103
1524.887749	57.920539	65.525108
1524.568471	40.634933	65.530113
1523.412525	47.857894	65.535118
1522.850808	56.722589	65.540122
1522.480927	46.017514	65.545127
1520.992609	55.010533	65.550132
1520.551910	52.360444	65.555137
1519.508423	54.248255	65.560142
1519.441328	50.654160	65.565146
1519.173256	46.991082	65.570151
1517.888375	48.655489	65.575156
1517.060840	45.935993	65.580161
1516.692965	45.863592	65.585166
1516.092718	43.672506	65.590170
1515.881967	38.152204	65.595175
1514.746248	50.194090	65.600180
1514.037459	46.853352	65.605185
1513.283338	45.210247	65.610190
1512.836056	43.887375	65.615194
1512.483595	34.122525	65.620199
1511.131915	47.148018	65.625204
1510.839945	36.299690	65.630209
1509.803793	48.273716	65.635214
1509.699381	46.022758	65.640218
1508.972057	37.309344	65.645223
1507.615097	47.841035	65.650228
1507.650016	40.416229	65.655233
1506.899822	43.421180	65.660238
1506.564547	42.995107	65.665242
1505.452181	50.162266	65.670247
1504.525458	40.914434	65.675252
1504.379183	35.111087	65.680257
1503.925801	48.036404	65.685262
1503.111916	48.952635	65.690266
1502.140558	44.713800	65.695271
1501.519225	45.414935	65.700276
1501.261036	47.919093	65.705281
1500.120591	49.314559	65.710286
1499.139180	44.213186	65.715290
1498.823535	35.161551	65.720295
1497.931449	55.993745	65.725300
1497.573059	40.384294	65.730305
1497.212987	46.553572	65.735310
1496.417859	42.677802	65.740314
1495.764292	39.538022	65.745319
1494.816086	46.814707	65.750324
1494.727415	35.617120	65.755329
1493.721603	45.216259	65.760334
1492.991343	41.699175	65.765338
1492.333751	36.620460	65.770343
1491.541976	44.452581	65.775348
1491.036184	33.896851	65.780353
1489.992621	49.878941	65.785358
1489.612006	37.587657	65.790362
1489.462893	42.310512	65.795367
1488.348554	40.890236	65.800372
1487.035298	40.704741	65.805377
1486.774896	51.563627	65.810382
1486.227252	49.250651	65.815386
1486.125597	38.507695	65.820391
1485.559230	45.961809	65.825396
1484.535202	36.749953	65.830401
1483.737209	39.805082	65.835406
1482.797626	41.583356	65.840410
1482.626023	41.941796	65.845415
1481.686411	47.495155	65.850420
1481.198360	44.221844	65.855425
1480.429012	46.696858	65.860430
1480.124521	44.376779	65.865434
1478.999521	39.378658	65.870439
1478.173717	43.691838	65.875444
1477.826217	45.150520	65.880449
1477.558835	43.045309	65.885454
1476.633619	37.379951	65.890458
1475.565487	41.761605	65.895463
1475.033828	45.061403	65.900468
1474.640915	47.746241	65.905473
1473.912537	47.731140	65.910478
1473.110909	47.705605	65.915482
1472.485463	49.875487	65.920487
1471.749363	44.214764	65.925492
1471.211938	41.390833	65.930497
1470.640508	56.607222	65.935502
1469.748261	49.427536	65.940506
1469.269300	41.746948	65.945511
1468.615634	45.774163	65.950516
1468.311078	47.312750	65.955521
1467.022031	42.979347	65.960526
1466.069256	46.932680	65.965530
1465.856236	43.727621	65.970535
1465.248843	50.216896	65.975540
1464.869289	42.003290	65.980545
1463.992237	55.264021	65.985550
1463.134788	46.891409	65.990554
1462.811323	42.373008	65.995559
1462.104836	48.969492	66.000564
1461.031261	35.723949	66.005569
1460.310110	51.530232	66.010574
1459.924105	51.250994	66.015578
1459.812313	35.438370	66.020583
1458.777584	55.129493	66.025588
1457.967822	50.199543	66.030593
1457.328406	49.457553	66.035598
1456.509438	51.667658	66.040602
1456.189159	58.467683	66.045607
1454.964214	57.008231	66.050612
1454.657628	43.686513	66.055617
1453.995517	53.171120	66.060622
1453.339212	42.084251	66.065626
1452.936446	39.330383	66.070631
1452.026140	52.866048	66.075636
1451.342307	48.160505	66.080641
1450.551103	48.040283	66.085646
1450.200760	42.750325	66.090650
1449.880265	36.878483	66.095655
1448.446208	39.854952	66.100660
1448.083863	51.518484	66.105665
1447.477101	53.450446	66.110670
1447.034651	44.508854	66.115674
1446.456227	46.909378	66.120679
1445.864726	53.009793	66.125684
1444.702736	47.438846	66.130689
1443.977715	41.956138	66.135694
1443.508465	52.558070	66.140698
1443.264581	41.610651	66.145703
1441.646042	42.739945	66.150708
1441.126044	47.786669	66.155713
1440.869212	49.644091	66.160718
1440.314823	39.226979	66.165722
1440.140169	37.469720	66.170727
1438.530167	56.096422	66.175732
1438.291167	44.582122	66.180737
1437.369710	52.840132	66.185742
1436.850313	45.221170	66.190746
1436.050231	55.577655	66.195751
1435.100759	46.789189	66.200756
1434.950604	40.779892	66.205761
1434.184583	46.660473	66.210766
1433.897069	49.770093	66.215770
1433.363474	51.904886	66.220775
1431.819266	52.793722	66.225780
1431.433902	46.083823	66.230785
1431.347199	44.989071	66.235790
1429.854516	44.095717	66.240794
1429.268119	41.326887	66.245799
1428.671428	45.482243	66.250804
1428.511357	48.927984	66.255809
1427.936578	52.742406	66.260814
1427.374313	53.098292	66.265818
1426.403046	43.949034	66.270823
1425.571034	54.420978	66.275828
1425.452040	50.185459	66.280833
1424.316117	44.435345	66.285838
1423.410816	45.711470	66.290842
1423.321674	42.120888	66.295847
1422.183691	51.916095	66.300852
1421.533847	56.065713	66.305857
1420.808562	56.747122	66.310862
1420.265989	56.443892	66.315866
1420.176027	42.321382	66.320871
1418.584855	54.462503	66.325876
1417.968460	42.670741	66.330881
1417.347184	49.436609	66.335886
1416.838076	49.279442	66.340890
1416.862898	43.485175	66.345895
1415.860121	53.057051	66.350900
1415.242061	47.525812	66.355905
1414.301320	51.141373	66.360910
1413.884121	46.253116	66.365914
1413.326423	44.733356	66.370919
1412.053739	52.336023	66.375924
1411.731741	40.820733	66.380929
1411.092429	48.302223	66.385934
1410.460716	53.571706	66.390938
1409.574788	49.805012	66.395943
1408.929029	52.194172	66.400948
1408.743043	47.212396	66.405953
1407.899385	53.176287	66.410958
1407.233486	46.424256	66.415962
1406.456293	44.050021	66.420967
1405.416889	55.926831	66.425972
1405.279654	54.564156	66.430977
1405.092622	51.793347	66.435982
1403.711270	41.936611	66.440986
1403.115887	44.275186	66.445991
1402.572880	52.793158	66.450996
1402.121182	48.787139	66.456001
1401.126356	45.233294	66.461006
1400.512359	49.760400	66.466010
1400.036261	45.546958	66.471015
1399.138238	50.910812	66.476020
1398.260702	46.314921	66.481025
1397.642075	52.919530	66.486030
1397.007698	52.402250	66.491034
1396.813741	45.885851	66.496039
1396.464584	48.924851	66.501044
1395.585882	51.699534	66.506049
1395.063477	47.640104	66.511054
1393.577535	38.984246	66.516058
1393.122856	48.216699	66.521063
1391.993249	45.695069	66.526068
1391.909013	42.759696	66.531073
1391.448523	42.831340	66.536078
1391.027896	42.002551	66.541082
1390.126356	42.868097	66.546087
1389.063648	49.336725	66.551092
1388.428371	50.241945	66.556097
1387.922801	49.842958	66.561102
1387.421262	39.002741	66.566106
1386.738330	35.277904	66.571111
1385.724197	51.228535	66.576116
1385.548733	42.747547	66.581121
1384.820468	42.032315	66.586126
1383.730800	42.311205	66.591130
1383.223856	38.443280	66.596135
1382.683759	47.627813	66.601140
1382.578763	36.492759	66.606145
1381.518127	41.149211	66.611150
1380.354664	38.632970	66.616154
1380.415502	41.471183	66.621159
1379.874511	42.730409	66.626164
1378.940919	48.271803	66.631169
1378.338336	41.230610	66.636174
1377.296725	44.374957	66.641178
1376.411806	40.023091	66.646183
1375.521006	39.013591	66.651188
1375.223924	43.789930	66.656193
1374.798380	34.993904	66.661198
1374.322760	38.866682	66.666202
1374.060701	29.622064	66.671207
1372.673793	43.526802	66.676212
1372.297278	34.816018	66.681217
1371.954112	37.546573	66.686222
1370.663799	43.929966	66.691226
1369.931274	39.873986	66.696231
1369.182512	34.401389	66.701236
1369.266240	29.813546	66.706241
1367.996482	44.130154	66.711246
1367.332129	39.665961	66.716250
1366.806351	34.683021	66.721255
1366.443354	45.173448	66.726260
1365.866700	33.009557	66.731265
1364.700753	49.949380	66.736270
1363.906939	37.804240	66.741274
1363.565429	45.490696	66.746279
1363.224377	46.289227	66.751284
1362.271477	51.513588	66.756289
1361.356574	38.831055	66.761294
1360.780189	54.795680	66.766298
1360.617271	44.702696	66.771303
1359.631626	48.139339	66.776308
1359.178426	51.579644	66.781313
1358.518724	37.654953	66.786318
1357.728594	44.766203	66.791322
1356.959064	40.500077	66.796327
1356.336160	45.807589	66.801332
1356.007496	46.451193	66.806337
1354.508326	47.944749	66.811342
1353.868177	53.374850	66.816346
1353.487684	43.956675	66.821351
1352.914470	49.589014	66.826356
1352.702612	44.888892	66.831361
1351.967171	51.592500	66.836366
1350.832089	51.061794	66.841370
1350.636428	40.414224	66.846375
1349.786099	45.248558	66.851380
1348.839609	39.662326	66.856385
1348.063126	57.156810	66.861390
1347.466697	54.009563	66.866394
1347.199544	33.973522	66.871399
1346.994869	53.720354	66.876404
1345.792653	54.602179	66.881409
1345.221184	44.009622	66.886414
1344.530182	47.872495	66.891418
1343.342253	37.053109	66.896423
1342.722614	53.614366	66.901428
1342.260467	39.098477	66.906433
1341.715829	46.110782	66.911438
1340.902183	38.196445	66.916442
1341.067202	43.615229	66.921447
1339.761924	53.284103	66.926452
1339.099945	34.279045	66.931457
1338.753861	49.607835	66.936462
1337.646755	48.981228	66.941466
1337.036229	33.188002	66.946471
1336.609570	49.803727	66.951476
1336.324182	49.997348	66.956481
1335.102272	43.691692	66.961486
1334.337281	52.563494	66.966490
1333.742775	41.635574	66.971495
1333.330465	39.622806	66.976500
1332.469617	41.973640	66.981505
1331.905451	47.036863	66.986510
1331.162622	45.278484	66.991514
1330.555581	39.116343	66.996519
1329.579693	51.634327	67.001524
1328.855295	46.127905	67.006529
1328.290831	51.046103	67.011534
1327.642642	45.302071	67.016538
1327.621601	42.074391	67.021543
1327.108376	45.560511	67.026548
1325.965931	45.344789	67.031553
1325.631056	49.934762	67.036558
1324.530588	46.224287	67.041562
1324.105184	44.890087	67.046567
1323.163926	49.608005	67.051572
1322.660840	34.038966	67.056577
1322.024275	43.554217	67.061582
1321.332774	45.252106	67.066586
1320.445149	35.015745	67.071591
1319.729200	52.707175	67.076596
1319.523705	21.720900	67.081601
1318.762549	35.442589	67.086606
1317.635695	46.398224	67.091610
1317.322798	30.724839	67.096615
1316.895558	42.117997	67.101620
1316.446729	28.617103	67.106625
1315.097366	29.246381	67.111630
1314.077005	31.887497	67.116634
1313.972370	25.246536	67.121639
1313.455524	42.966221	67.126644
1312.899328	28.638763	67.131649
1312.307056	34.909619	67.136654
1311.554878	38.804300	67.141658
1311.146061	32.839300	67.146663
1309.769040	34.573646	67.151668
1309.314130	40.232908	67.156673
1308.872469	39.446900	67.161678
1308.330212	35.616146	67.166682
1307.683669	28.142020	67.171687
1306.671816	39.651779	67.176692
1306.192784	37.900350	67.181697
1305.111454	36.397641	67.186702
1304.029975	28.319336	67.191706
1303.966829	33.771235	67.196711
1303.308279	35.848649	67.201716
1303.242208	35.203190	67.206721
1302.674438	32.901345	67.211726
1301.469191	48.253199	67.216730
1301.034591	36.806303	67.221735
1300.207249	51.249710	67.226740
1299.510936	38.726410	67.231745
1298.702068	34.482328	67.236750
1298.146326	35.042200	67.241754
1298.024735	22.525303	67.246759
1296.582886	34.119198	67.251764
1295.536189	31.660124	67.256769
1295.048121	37.465002	67.261774
1294.807514	34.967644	67.266778
1295.086525	41.614039	67.271783
1293.826665	33.909437	67.276788
1292.957479	29.447878	67.281793
1292.352492	31.578276	67.286798
1291.546028	38.619599	67.291802
1290.960802	25.681275	67.296807
1290.243235	38.621790	67.301812
1289.699060	34.092785	67.306817
1289.303239	36.405960	67.311822
1287.834375	37.667662	67.316826
1287.833512	31.746609	67.321831
1286.873022	39.968282	67.326836
1286.496284	40.627423	67.331841
1285.533623	26.761981	67.336846
1284.446855	39.937812	67.341850
1284.198286	28.477118	67.346855
1283.890433	29.431221	67.351860
1283.299884	24.608409	67.356865
1282.205498	29.536754	67.361870
1281.638491	34.881118	67.366874
1281.198039	37.351195	67.371879
1279.901559	45.074387	67.376884
1279.507138	34.160407	67.381889
1278.953556	32.184305	67.386894
1278.566240	31.564696	67.391898
1278.559042	26.573439	67.396903
1277.088161	38.496800	67.401908
1276.398864	34.101256	67.406913
1275.696788	38.546197	67.411918
1274.431112	38.066253	67.416922
1274.116435	36.389618	67.421927
1273.314585	36.600714	67.426932
1272.889301	31.609704	67.431937
1272.981069	31.475291	67.436942
1271.957925	40.662524	67.441946
1271.327083	23.901203	67.446951
1270.497088	43.868861	67.451956
1270.120134	43.066263	67.456961
1268.903241	37.482064	67.461966
1268.354765	39.598752	67.466970
1268.394179	34.573274	67.471975
1267.216224	43.080258	67.476980
1266.248227	38.744800	67.481985
1265.954482	38.198620	67.486990
1265.477441	35.502328	67.491994
1264.465373	34.184158	67.496999
1263.324821	40.557974	67.502004
1263.158295	37.353433	67.507009
1262.676739	30.986867	67.512014
1262.042192	44.052955	67.517018
1261.207817	36.685974	67.522023
1260.264720	42.362949	67.527028
1259.924196	42.130124	67.532033
1259.655744	31.144084	67.537038
1258.374413	32.319214	67.542042
1257.639118	30.890808	67.547047
1256.769428	41.781913	67.552052
1256.795296	34.368028	67.557057
1256.272155	31.604955	67.562062
1255.118203	31.761663	67.567066
1254.651042	29.013343	67.572071
1254.249436	32.193153	67.577076
1253.763415	32.641026	67.582081
1252.746293	34.157330	67.587086
1252.137078	41.104223	67.592090
1251.033142	20.013898	67.597095
1250.175867	41.256862	67.602100
1249.554854	30.186545	67.607105
1249.247311	35.743535	67.612110
1248.879512	40.967924	67.617114
1248.629061	33.079184	67.622119
1247.354038	39.091206	67.627124
1247.044670	41.847937	67.632129
1245.575377	46.301352	67.637134
1244.871728	34.794761	67.642138
1244.335347	41.637037	67.647143
1243.957614	37.169881	67.652148
1243.602586	31.734063	67.657153
1243.096637	33.334657	67.662158
1241.641674	37.189730	67.667162
1241.352234	45.678432	67.672167
1240.995831	47.908080	67.677172
1240.313048	32.679873	67.682177
1239.600863	33.527974	67.687182
1238.672269	32.931370	67.692186
1238.486796	25.669365	67.697191
1237.168853	33.709781	67.702196
1236.737400	30.189419	67.707201
1236.224362	26.473883	67.712206
1235.653350	36.934311	67.717210
1234.652560	35.574937	67.722215
1233.558821	43.822548	67.727220
1233.630298	31.058920	67.732225
1232.906179	37.041686	67.737230
1232.236276	41.360102	67.742234
1231.475452	31.158812	67.747239
1230.633317	35.834185	67.752244
1230.544032	35.749060	67.757249
1229.635393	31.009960	67.762254
1228.608042	32.821200	67.767258
1228.437670	28.079812	67.772263
1227.722382	34.959999	67.777268
1226.826962	33.743138	67.782273
1226.229233	34.601426	67.787278
1225.555589	36.589799	67.792282
1225.122027	31.368314	67.797287
1223.728414	35.407597	67.802292
1223.205221	28.582482	67.807297
1222.922251	34.753705	67.812302
1222.312474	39.037330	67.817306
1222.046718	31.508983	67.822311
1220.988946	34.930334	67.827316
1220.209179	31.862742	67.832321
1219.981394	26.231660	67.837326
1218.739301	32.889709	67.842330
1217.836963	19.959271	67.847335
1217.128661	38.002698	67.852340
1216.890027	34.580980	67.857345
1216.570942	32.976015	67.862350
1215.693024	36.917523	67.867354
1215.068078	35.761727	67.872359
1214.279654	39.051942	67.877364
1213.906408	37.816696	67.882369
1212.792687	36.976741	67.887374
1211.930290	38.482647	67.892378
1211.657398	30.037689	67.897383
1211.133738	40.083754	67.902388
1210.639816	36.639560	67.907393
1210.001654	40.688016	67.912398
1208.983595	44.733813	67.917402
1208.931745	40.560176	67.922407
1207.595269	38.736979	67.927412
1206.709115	39.770445	67.932417
1206.429819	39.806999	67.937422
1205.815676	35.962473	67.942426
1204.996331	29.244383	67.947431
1204.108514	33.442923	67.952436
1203.707780	44.809796	67.957441
1203.559815	34.635624	67.962446
1202.112122	33.060344	67.967450
1201.625843	34.178445	67.972455
1200.746691	40.133837	67.977460
1200.766422	35.816360	67.982465
1200.127115	34.859963	67.987470
1199.004317	36.183368	67.992474
1198.722359	30.994547	67.997479
1197.850755	41.632091	68.002484
1197.005883	35.913076	68.007489
1196.274342	31.153709	68.012494
1195.787651	34.782278	68.017498
1195.630495	26.170692	68.022503
1194.351119	30.858843	68.027508
1194.036008	35.688518	68.032513
1193.363109	33.693567	68.037518
1192.526020	37.264328	68.042522
1191.503722	34.933878	68.047527
1190.740669	27.837850	68.052532
1190.278671	30.595205	68.057537
1190.050436	32.530094	68.062542
1189.359982	26.840141	68.067546
1188.340639	31.825970	68.072551
1187.665084	33.896653	68.077556
1187.525949	27.699568	68.082561
1186.928050	33.406813	68.087566
1185.603257	35.866169	68.092570
1185.115253	27.928495	68.097575
1184.524198	39.989502	68.102580
1184.385336	29.052254	68.107585
1183.510374	39.346573	68.112590
1182.823983	33.118255	68.117594
1182.499323	35.131556	68.122599
1180.971607	42.517842	68.127604
1180.311766	38.161796	68.132609
1179.997823	35.083206	68.137614
1179.399741	31.217212	68.142618
1178.331118	31.156966	68.147623
1177.592248	45.080135	68.152628
1177.333890	41.945397	68.157633
1177.137879	35.929235	68.162638
1175.956087	31.629398	68.167642
1175.266148	31.455311	68.172647
1174.623076	48.759859	68.177652
1174.387649	38.735212	68.182657
1173.743209	38.937072	68.187662
1172.203899	49.188835	68.192666
1171.935735	35.558326	68.197671
1171.126501	35.486789	68.202676
1170.853266	34.492677	68.207681
1169.999987	33.721700	68.212686
1169.181481	41.528181	68.217690
1168.933285	32.301898	68.222695
1167.926245	47.340004	68.227700
1167.518895	32.999961	68.232705
1166.934913	36.934156	68.237710
1166.151500	46.665168	68.242714
1165.980965	37.957940	68.247719
1164.742478	33.085255	68.252724
1163.961236	32.119904	68.257729
1163.691022	30.902972	68.262734
1162.652752	39.487120	68.267738
1161.950962	29.527195	68.272743
1161.192274	34.012703	68.277748
1160.886187	28.996454	68.282753
1160.543027	32.512317	68.287758
1159.446343	34.358264	68.292762
1158.615172	28.039449	68.297767
1157.974111	30.658140	68.302772
1157.565362	37.664621	68.307777
1157.046864	34.011469	68.312782
1155.811989	37.399516	68.317786
1155.548050	26.698201	68.322791
1155.006253	32.374452	68.327796
1153.973309	32.988178	68.332801
1153.141788	33.435832	68.337806
1152.645478	33.311376	68.342810
1152.477478	28.832958	68.347815
1151.912369	37.677727	68.352820
1151.131650	20.563425	68.357825
1150.271510	28.518445	68.362830
1149.917588	36.006617	68.367834
1149.301589	27.936354	68.372839
1148.153978	32.223538	68.377844
1147.604249	38.205393	68.382849
1146.902420	36.465781	68.387854
1146.035776	31.425158	68.392858
1145.271263	36.206474	68.397863
1144.913537	42.055294	68.402868
1144.264990	41.265953	68.407873
1144.276146	34.464671	68.412878
1143.030920	38.861999	68.417882
1142.709283	33.343622	68.422887
1141.733746	44.861845	68.427892
1140.262287	43.788676	68.432897
1140.039333	35.991770	68.437902
1139.198736	39.184653	68.442906
1139.232334	29.309609	68.447911
1138.801537	38.256012	68.452916
1138.062981	30.370818	68.457921
1137.220276	32.446024	68.462926
1136.493008	39.019068	68.467930
1135.727206	34.082251	68.472935
1134.724333	25.233051	68.477940
1134.602883	41.811254	68.482945
1133.997634	31.167384	68.487950
1132.796371	37.140915	68.492954
1132.027414	35.159684	68.497959
1131.178536	38.603034	68.502964
1131.471613	38.271021	68.507969
1131.231052	30.574688	68.512974
1129.686661	36.255884	68.517978
1129.645678	24.943550	68.522983
1128.317909	40.792732	68.527988
1127.347802	34.339914	68.532993
1127.035933	25.212078	68.537998
1126.116187	40.819748	68.543002
1126.099812	28.719786	68.548007
1125.351654	39.198943	68.553012
1124.521428	37.329956	68.558017
1124.085233	37.205404	68.563022
1123.224741	37.290262	68.568026
1122.190932	27.826272	68.573031
1121.454072	28.023923	68.578036
1120.854912	39.170056	68.583041
1120.626237	28.336988	68.588046
1119.953339	33.073776	68.593050
1119.394462	29.584746	68.598055
1118.406229	27.807126	68.603060
1118.151863	25.598972	68.608065
1117.488442	37.643111	68.613070
1115.783639	38.586064	68.618074
1115.720921	34.235977	68.623079
1115.293813	35.847707	68.628084
1115.075283	35.018357	68.633089
1114.241066	33.105857	68.638094
1113.137303	34.487769	68.643098
1112.823440	34.616560	68.648103
1112.157710	31.642824	68.653108
1111.144555	33.688384	68.658113
1111.011421	41.404779	68.663118
1109.714150	45.950746	68.668122
1108.823708	37.124665	68.673127
1108.186470	43.582475	68.678132
1107.632712	33.646328	68.683137
1107.345652	30.290674	68.688142
1106.914623	44.688409	68.693146
1106.620799	34.266232	68.698151
1105.702401	35.669121	68.703156
1104.960390	33.909106	68.708161
1103.859161	38.368697	68.713166
1103.124000	41.089099	68.718170
1102.745431	32.918004	68.723175
1101.786908	45.679270	68.728180
1101.309550	28.253388	68.733185
1100.782083	29.857431	68.738190
1099.786480	35.121776	68.743194
1099.703846	24.472056	68.748199
1098.988934	46.638526	68.753204
1098.611778	29.542042	68.758209
1097.893746	32.325948	68.763214
1096.620507	35.899888	68.768218
1096.052941	29.023522	68.773223
1095.358711	29.777347	68.778228
1094.762234	30.227053	68.783233
1093.811892	36.242682	68.788238
1093.031430	41.512230	68.793242
1092.512061	36.460536	68.798247
1091.902586	39.925735	68.803252
1091.526900	39.184463	68.808257
1091.357785	32.183214	68.813262
1090.155365	43.568815	68.818266
1089.175442	25.193182	68.823271
1089.050037	41.636396	68.828276
1088.215789	36.920209	68.833281
1087.467221	38.438008	68.838286
1086.679044	50.506738	68.843290
1086.389386	36.313569	68.848295
1085.818299	42.257833	68.853300
1084.694069	36.040854	68.858305
1084.326098	31.061269	68.863310
1083.765817	33.630858	68.868314
1083.010617	35.958654	68.873319
1081.954461	23.716619	68.878324
1081.483066	50.543467	68.883329
1081.250048	30.317594	68.888334
1079.918151	29.012534	68.893338
1079.618771	31.428660	68.898343
1078.760486	39.105877	68.903348
1078.483230	22.843455	68.908353
1077.859266	29.806909	68.913358
1076.720007	35.332225	68.918362
1076.565428	27.977024	68.923367
1075.706561	37.800471	68.928372
1074.539501	37.246595	68.933377
1073.951428	28.192669	68.938382
1073.397922	27.981136	68.943386
1072.944884	43.730607	68.948391
1072.635464	31.084360	68.953396
1071.712939	29.193809	68.958401
1071.150075	20.916435	68.963406
1070.251585	29.613980	68.968410
1069.898692	30.289857	68.973415
1068.598904	33.677230	68.978420
1068.265960	22.062863	68.983425
1068.061790	23.085647	68.988430
1066.816926	24.277146	68.993434
1066.124024	24.480435	68.998439
1065.640672	44.771420	69.003444
1065.138843	13.302582	69.008449
1065.083934	24.980264	69.013454
1063.688755	35.094028	69.018458
1063.408018	24.773860	69.023463
1062.369970	30.461266	69.028468
1061.474796	23.093008	69.033473
1060.976423	21.035640	69.038478
1060.080353	28.021886	69.043482
1060.151885	28.038911	69.048487
1059.375738	30.770574	69.053492
1058.242977	35.339272	69.058497
1057.923314	24.044477	69.063502
1057.284475	35.758297	69.068506
1056.682737	25.884996	69.073511
1056.232574	28.087002	69.078516
1055.175992	27.936587	69.083521
1054.444478	28.000949	69.088526
1053.404490	34.876061	69.093530
1053.139175	17.295055	69.098535
1052.513947	31.294761	69.103540
1052.083653	20.104300	69.108545
1051.236639	21.475351	69.113550
1050.538893	33.466611	69.118554
1049.706439	33.192235	69.123559
1048.755116	38.077410	69.128564
1048.271218	35.175684	69.133569
1047.657337	30.779254	69.138574
1046.822059	33.573942	69.143578
1046.995624	25.496364	69.148583
1046.506096	29.899655	69.153588
1045.349527	30.520478	69.158593
1044.774612	34.486367	69.163598
1043.635105	31.532836	69.168602
1042.957177	30.245172	69.173607
1042.219904	32.335172	69.178612
1042.169740	22.616964	69.183617
1041.812980	32.352648	69.188622
1040.558867	31.230768	69.193626
1039.988967	28.864676	69.198631
1039.543457	27.809683	69.203636
1038.544795	39.003615	69.208641
1037.768763	21.349329	69.213646
1036.944514	31.632454	69.218650
1036.666729	32.996521	69.223655
1036.115289	37.920577	69.228660
1035.094325	38.436255	69.233665
1034.435933	40.993080	69.238670
1033.739726	43.981680	69.243674
1033.468534	35.984320	69.248679
1033.264029	32.028941	69.253684
1032.160376	29.293629	69.258689
1031.228987	35.066576	69.263694
1030.891263	40.727726	69.268698
1029.968351	31.197253	69.273703
1029.019155	36.777501	69.278708
1028.454460	38.343329	69.283713
1028.085760	34.081352	69.288718
1027.813396	37.767306	69.293722
1026.797622	39.166793	69.298727
1025.980752	31.571632	69.303732
1025.373828	39.656706	69.308737
1024.820694	35.472956	69.313742
1023.923588	43.151636	69.318746
1023.548623	36.657789	69.323751
1022.997559	32.439020	69.328756
1022.314989	37.722970	69.333761
1021.634435	30.686416	69.338766
1020.867073	36.510536	69.343770
1020.284632	31.021062	69.348775
1019.567958	45.352288	69.353780
1018.888975	37.809301	69.358785
1018.438677	37.933005	69.363790
1017.231983	40.695338	69.368794
1016.573176	29.796693	69.373799
1015.802194	33.114147	69.378804
1015.746869	33.704840	69.383809
1015.614602	26.025991	69.388814
1014.581306	29.391488	69.393818
1013.816770	32.230120	69.398823
1012.497811	25.919592	69.403828
1011.542092	31.060931	69.408833
1011.249946	25.832766	69.413838
1010.520208	38.396803	69.418842
1010.702943	33.044194	69.423847
1010.133366	40.885219	69.428852
1009.013295	39.825601	69.433857
1008.388475	29.405655	69.438862
1007.288162	37.365815	69.443866
1006.703863	29.218018	69.448871
1005.841798	40.224654	69.453876
1005.401365	49.568405	69.458881
1005.388219	31.991426	69.463886
1004.549348	28.879698	69.468890
1003.609606	40.797517	69.473895
1003.064128	36.271948	69.478900
1002.503435	30.701752	69.483905
1001.776628	20.354810	69.488910
1000.442661	49.939670	69.493914
999.938802	36.140137	69.498919
999.661017	38.854020	69.503924
999.076021	35.520556	69.508929
998.622926	34.419470	69.513934
997.577723	38.099092	69.518938
997.392574	29.001580	69.523943
996.363103	44.700851	69.528948
995.515548	35.057481	69.533953
995.244525	21.977819	69.538958
994.168366	47.880637	69.543962
993.582586	32.794792	69.548967
992.814023	35.116855	69.553972
992.211514	29.318360	69.558977
991.498013	27.322044	69.563982
991.293209	39.983901	69.568986
990.497967	32.694382	69.573991
989.817483	31.974817	69.578996
989.157737	34.441985	69.584001
988.824820	26.178505	69.589006
987.553279	47.878488	69.594010
986.958815	29.310696	69.599015
986.423745	25.800568	69.604020
985.868674	35.916301	69.609025
985.122918	30.317213	69.614030
984.226780	34.454069	69.619034
983.919862	26.363065	69.624039
983.578534	31.482341	69.629044
982.493130	34.457191	69.634049
981.758722	27.758789	69.639054
981.068724	34.723308	69.644058
981.041009	31.810508	69.649063
979.985207	33.836096	69.654068
979.321759	29.627338	69.659073
978.520385	31.117301	69.664078
977.588414	31.532113	69.669082
977.061824	30.059544	69.674087
976.663883	25.209326	69.679092
975.954388	25.916728	69.684097
975.153368	25.665759	69.689102
974.307452	27.951250	69.694106
973.663731	30.967780	69.699111
973.356237	38.615724	69.704116
972.848864	41.416603	69.709121
972.133462	25.772683	69.714126
971.119157	28.048703	69.719130
970.865979	25.695306	69.724135
969.773497	32.752255	69.729140
969.010823	36.858417	69.734145
968.851596	29.940766	69.739150
968.182252	30.424172	69.744154
967.140889	29.875574	69.749159
966.492316	29.791152	69.754164
966.016216	22.316828	69.759169
965.687675	19.868197	69.764174
964.403902	39.419256	69.769178
963.650414	32.124680	69.774183
963.475414	33.051371	69.779188
962.856955	26.288797	69.784193
962.284646	25.597756	69.789198
961.315055	29.430930	69.794202
960.883804	38.054158	69.799207
959.761588	37.152592	69.804212
958.484342	40.102790	69.809217
958.509792	32.633803	69.814222
957.743739	44.427807	69.819226
957.703446	35.250478	69.824231
957.427756	30.596841	69.829236
956.179263	35.731174	69.834241
955.580227	34.186564	69.839246
954.902065	30.213533	69.844250
954.124989	29.085168	69.849255
953.389205	28.412259	69.854260
952.677515	40.661212	69.859265
952.470026	31.530993	69.864270
951.051648	39.619055	69.869274
950.660928	31.356896	69.874279
950.169054	34.278307	69.879284
949.568027	40.731959	69.884289
948.644356	34.431098	69.889294
947.655746	37.576631	69.894298
947.777943	33.014211	69.899303
947.570473	37.456208	69.904308
946.041933	37.095528	69.909313
945.688752	27.576930	69.914318
944.879483	37.006179	69.919322
944.078549	36.283718	69.924327
943.220272	37.207186	69.929332
942.709659	32.732854	69.934337
942.403293	25.185795	69.939342
941.749018	35.774616	69.944346
940.958520	26.680412	69.949351
940.137288	33.276332	69.954356
939.442674	45.700762	69.959361
939.373420	39.645539	69.964366
937.905994	35.777614	69.969370
937.178363	26.591410	69.974375
936.943424	24.496877	69.979380
936.111250	45.237589	69.984385
935.551429	17.765977	69.989390
934.644199	34.879182	69.994394
934.093683	31.615940	69.999399
933.733006	24.853352	70.004404
933.446685	22.792226	70.009409
932.352981	19.801502	70.014414
931.706601	30.854244	70.019418
931.431501	20.444906	70.024423
930.483781	27.299065	70.029428
929.460959	33.069247	70.034433
929.198357	37.084799	70.039438
928.062437	22.755138	70.044442
927.465756	11.654275	70.049447
926.763830	37.726176	70.054452
926.583113	31.329167	70.059457
926.293346	22.158438	70.064462
924.628326	35.010094	70.069466
924.566857	34.466413	70.074471
924.016119	26.660217	70.079476
922.757004	18.708151	70.084481
922.086959	22.451089	70.089486
921.563891	33.263447	70.094490
921.428670	23.412141	70.099495
920.730519	27.750884	70.104500
919.880885	41.742172	70.109505
919.014395	23.225594	70.114510
918.361471	36.876504	70.119514
917.494727	28.641228	70.124519
916.810067	36.038552	70.129524
916.232812	30.166679	70.134529
916.170099	30.277601	70.139534
915.290948	30.982060	70.144538
914.515695	36.082095	70.149543
913.907432	35.210715	70.154548
913.196351	32.025069	70.159553
912.363272	22.239099	70.164558
911.411841	27.505936	70.169562
911.521437	33.341895	70.174567
910.766736	35.743772	70.179572
909.697405	30.686617	70.184577
908.926469	26.822980	70.189582
908.590283	38.638456	70.194586
908.169646	27.724026	70.199591
907.079995	28.783672	70.204596
906.232810	34.253109	70.209601
906.068124	36.956883	70.214606
905.272526	27.262714	70.219610
904.456638	31.028870	70.224615
903.732344	13.355389	70.229620
903.016069	26.767227	70.234625
903.157796	37.016490	70.239630
901.712016	31.823718	70.244634
900.934983	31.092737	70.249639
900.258509	23.743357	70.254644
899.959521	37.278018	70.259649
899.666830	12.865645	70.264654
898.606580	37.409811	70.269658
897.909295	31.968611	70.274663
897.491876	27.345426	70.279668
896.388025	42.640260	70.284673
895.822781	34.757532	70.289678
895.288729	41.369260	70.294682
894.948593	22.168133	70.299687
893.827473	25.374194	70.304692
892.857971	42.163027	70.309697
892.364585	24.227294	70.314702
892.097486	36.399186	70.319706
891.537256	20.946645	70.324711
891.162910	27.660676	70.329716
890.266605	24.961814	70.334721
889.697296	12.163039	70.339726
888.758071	31.285552	70.344730
888.274077	28.779675	70.349735
887.773998	28.420915	70.354740
886.455797	19.120581	70.359745
886.063459	24.711584	70.364750
885.428354	30.126771	70.369754
884.965881	23.435587	70.374759
883.462924	32.309809	70.379764
882.972857	34.095591	70.384769
882.667331	25.484016	70.389774
881.957413	31.901392	70.394778
881.810843	24.489755	70.399783
880.794967	25.228601	70.404788
879.855442	26.376323	70.409793
879.891475	23.847602	70.414798
878.928121	29.001236	70.419802
877.865429	27.850549	70.424807
877.267733	28.507070	70.429812
876.841547	31.090047	70.434817
876.474362	22.075147	70.439822
875.188605	27.995999	70.444826
874.617724	41.138719	70.449831
874.304580	32.985650	70.454836
873.733958	33.393447	70.459841
872.805210	20.754377	70.464846
872.022626	15.102853	70.469850
871.458906	26.058868	70.474855
871.059535	28.788957	70.479860
870.186743	22.771760	70.484865
869.780050	19.313766	70.489870
868.739379	31.829542	70.494874
868.464225	24.170303	70.499879
867.703476	20.048030	70.504884
866.879901	27.159978	70.509889
866.324364	38.095777	70.514894
865.762104	36.997901	70.519898
864.766776	32.717428	70.524903
864.232107	30.569690	70.529908
863.747486	37.791689	70.534913
863.237588	22.812095	70.539918
862.022492	35.456559	70.544922
861.564910	25.180353	70.549927
861.054524	34.413819	70.554932
859.832150	39.592922	70.559937
859.231327	26.587860	70.564942
858.490563	35.476391	70.569946
858.048829	35.778524	70.574951
857.975902	29.183028	70.579956
857.383416	28.250807	70.584961
856.941814	25.889571	70.589966
855.819535	37.502178	70.594970
855.041731	38.338752	70.599975
854.250362	44.920485	70.604980
853.550939	24.548167	70.609985
853.584986	25.018987	70.614990
852.675864	29.771354	70.619994
851.913733	24.174923	70.624999
851.254769	25.238575	70.630004
849.839330	24.301736	70.635009
849.456121	24.862624	70.640014
848.520335	25.612388	70.645018
848.088745	21.705797	70.650023
848.183739	21.189250	70.655028
847.129235	35.161118	70.660033
846.703193	25.324577	70.665038
845.981247	31.731260	70.670042
845.416215	36.195484	70.675047
844.405117	26.406339	70.680052
843.677686	34.969490	70.685057
843.357810	26.016448	70.690062
842.158174	27.850530	70.695066
841.502350	29.165986	70.700071
841.018961	30.941250	70.705076
840.513783	27.461091	70.710081
840.155028	20.639875	70.715086
839.190781	33.747440	70.720090
838.797491	28.642631	70.725095
838.142667	25.999963	70.730100
837.229559	34.479136	70.735105
836.601681	24.351465	70.740110
836.244261	31.572140	70.745114
834.926646	32.024736	70.750119
833.917178	23.589878	70.755124
833.248940	32.667132	70.760129
833.065043	32.516661	70.765134
832.532993	40.170396	70.770138
832.346098	32.219580	70.775143
831.605678	40.810035	70.780148
830.478756	35.085602	70.785153
830.119168	22.160421	70.790158
829.299142	31.646595	70.795162
828.169246	30.457743	70.800167
827.631416	30.850869	70.805172
827.471223	30.594128	70.810177
827.337021	23.052804	70.815182
825.933656	35.061806	70.820186
825.479873	21.686442	70.825191
824.925162	21.752687	70.830196
823.382468	26.422999	70.835201
822.938619	22.698128	70.840206
822.602197	29.015062	70.845210
822.311037	28.471679	70.850215
821.204194	25.770089	70.855220
820.429226	27.550772	70.860225
820.090439	26.351105	70.865230
819.777993	23.507291	70.870234
818.925290	24.586023	70.875239
818.213268	18.648908	70.880244
817.289167	25.474110	70.885249
816.904613	19.573172	70.890254
815.541832	29.500543	70.895258
814.956538	19.189496	70.900263
814.519448	27.482513	70.905268
813.902363	32.021256	70.910273
813.785543	22.848251	70.915278
812.827085	25.000327	70.920282
811.932883	21.137425	70.925287
811.811868	18.324639	70.930292
810.661393	28.790622	70.935297
810.100645	25.752959	70.940302
809.242943	33.264576	70.945306
808.990680	34.307650	70.950311
808.299942	27.056761	70.955316
807.381537	17.949865	70.960321
806.771226	27.084127	70.965326
806.207462	36.045412	70.970330
805.635757	36.060753	70.975335
804.764619	31.883534	70.980340
804.406534	31.598377	70.985345
803.956671	9.928028	70.990350
802.595101	26.858119	70.995354
801.886304	32.209364	71.000359
801.667576	21.956653	71.005364
800.679464	28.441985	71.010369
800.100762	20.581937	71.015374
799.343116	27.153576	71.020378
799.059516	21.403719	71.025383
798.688590	22.085656	71.030388
797.275759	27.906929	71.035393
796.969187	18.710522	71.040398
796.206590	34.045661	71.045402
795.961963	24.788929	71.050407
794.700604	34.394253	71.055412
793.830124	28.092879	71.060417
793.940067	29.551356	71.065422
792.824161	32.296182	71.070426
791.817362	32.639399	71.075431
791.691284	30.120718	71.080436
790.997684	34.745760	71.085441
790.590980	31.669385	71.090446
789.336121	29.033949	71.095450
788.628079	29.644982	71.100455
788.391235	33.300067	71.105460
787.449280	34.165948	71.110465
787.312058	26.325500	71.115470
786.415678	35.893224	71.120474
785.797180	29.192210	71.125479
785.133960	29.789801	71.130484
784.169595	31.327846	71.135489
783.824963	28.017675	71.140494
783.122685	19.939198	71.145498
782.405655	21.879394	71.150503
781.733804	29.408735	71.155508
780.864941	24.488457	71.160513
780.621527	22.075185	71.165518
779.715162	28.329900	71.170522
778.754655	31.485210	71.175527
778.310069	16.760171	71.180532
777.636282	26.021231	71.185537
777.493042	19.911581	71.190542
776.400725	20.438722	71.195546
775.392556	21.808710	71.200551
774.951504	22.724154	71.205556
774.574591	30.108776	71.210561
773.828633	16.720028	71.215566
772.755732	32.293794	71.220570
772.397897	23.121320	71.225575
772.251609	19.170902	71.230580
771.115602	24.265328	71.235585
770.466984	23.823012	71.240590
769.644966	31.939210	71.245594
769.485078	23.921034	71.250599
768.714115	15.148636	71.255604
767.900652	28.825113	71.260609
767.414435	13.073855	71.265614
766.106281	16.251399	71.270618
765.229102	25.317772	71.275623
765.147252	23.686141	71.280628
764.794891	24.757770	71.285633
764.327018	23.179712	71.290638
763.174021	24.506535	71.295642
762.625476	20.553930	71.300647
762.373083	16.990972	71.305652
761.171495	21.638548	71.310657
760.500770	26.389256	71.315662
760.281925	32.457253	71.320666
759.191485	24.183550	71.325671
758.522386	22.782603	71.330676
757.678364	21.165091	71.335681
757.505636	17.819673	71.340686
756.405217	14.830102	71.345690
755.638226	19.892589	71.350695
755.037517	14.830287	71.355700
754.371600	18.511108	71.360705
754.259489	20.791796	71.365710
753.283141	22.314414	71.370714
752.456712	19.998700	71.375719
752.118266	24.712276	71.380724
751.943365	18.502020	71.385729
750.777871	13.017157	71.390734
749.937382	28.326852	71.395738
749.334258	26.962710	71.400743
748.880121	25.626885	71.405748
747.452663	28.492291	71.410753
747.257166	17.721834	71.415758
746.901680	22.365587	71.420762
746.326583	14.333106	71.425767
745.505908	24.336612	71.430772
744.602568	30.065756	71.435777
744.244979	20.634643	71.440782
742.935183	25.408261	71.445786
742.165643	31.983386	71.450791
741.775455	26.312006	71.455796
741.857006	26.313235	71.460801
741.183916	11.353373	71.465806
739.800696	22.566026	71.470810
739.346677	29.734280	71.475815
739.166554	24.060994	71.480820
737.876433	29.938450	71.485825
737.291136	23.850304	71.490830
736.981315	28.423713	71.495834
736.485500	23.686896	71.500839
735.562485	19.844381	71.505844
734.473037	22.708013	71.510849
734.245614	14.699024	71.515854
733.673151	22.494807	71.520858
732.690224	25.576435	71.525863
732.110570	24.541282	71.530868
731.238067	21.922266	71.535873
731.323988	21.460774	71.540878
730.017738	24.753147	71.545882
729.489873	24.211195	71.550887
728.771439	18.841231	71.555892
728.376192	23.362013	71.560897
727.627131	17.534901	71.565902
726.747678	19.324363	71.570906
726.196911	25.131407	71.575911
726.058351	21.883049	71.580916
724.589491	36.042345	71.585921
724.138672	17.472312	71.590926
723.639415	21.724240	71.595930
723.236017	16.416076	71.600935
722.449641	22.766812	71.605940
721.491987	19.749794	71.610945
721.363608	20.818879	71.615950
719.839635	19.886781	71.620954
719.114837	29.173320	71.625959
718.953820	18.026812	71.630964
718.460374	33.237107	71.635969
718.130086	33.119416	71.640974
716.743696	27.291286	71.645978
716.085809	30.191862	71.650983
715.624721	14.890761	71.655988
715.088509	28.314953	71.660993
714.313201	19.201084	71.665998
713.449550	25.546783	71.671002
712.888862	23.034235	71.676007
712.362358	24.231364	71.681012
711.573266	33.561260	71.686017
710.904652	19.452203	71.691022
710.306321	27.125961	71.696026
710.036484	27.943194	71.701031
709.330360	33.681947	71.706036
708.358432	27.768906	71.711041
707.892563	24.686201	71.716046
707.353695	28.613296	71.721050
706.248397	29.940434	71.726055
705.639014	24.791220	71.731060
705.102036	30.802645	71.736065
704.635796	18.432201	71.741070
703.762567	30.751057	71.746074
702.921832	29.607679	71.751079
702.794756	25.029764	71.756084
701.677147	22.867660	71.761089
700.530474	20.360119	71.766094
700.016947	22.933373	71.771098
699.604442	27.832204	71.776103
699.462595	20.974902	71.781108
698.527075	35.233778	71.786113
697.735003	28.234018	71.791118
697.036151	42.783205	71.796122
696.644702	29.358529	71.801127
696.545305	17.380661	71.806132
695.244946	23.357531	71.811137
694.855438	21.796970	71.816142
693.618782	34.865950	71.821146
693.191850	28.358379	71.826151
692.551460	33.285615	71.831156
691.674941	32.209437	71.836161
691.079880	28.890276	71.841166
690.280532	31.750309	71.846170
689.868009	29.322978	71.851175
689.490434	26.970502	71.856180
688.743154	26.173353	71.861185
687.885607	32.150677	71.866190
687.473014	31.073163	71.871194
686.804004	22.681932	71.876199
685.641155	20.214818	71.881204
684.802737	46.560767	71.886209
684.533883	26.238235	71.891214
684.008641	24.458028	71.896218
683.326506	19.951158	71.901223
683.005116	16.345584	71.906228
682.009514	35.496035	71.911233
681.783258	22.157023	71.916238
680.939661	29.258015	71.921242
680.292226	28.918032	71.926247
679.259659	19.026745	71.931252
678.007503	24.970717	71.936257
677.976511	24.042164	71.941262
677.174962	29.122791	71.946266
676.654199	29.230970	71.951271
676.468866	27.882314	71.956276
675.119276	33.534316	71.961281
674.550199	29.179744	71.966286
674.090501	18.159651	71.971290
673.313080	37.269055	71.976295
672.526750	20.564298	71.981300
671.721303	29.133596	71.986305
671.488688	25.457117	71.991310
671.136624	26.451444	71.996314
670.555170	34.710699	72.001319
669.659912	25.256418	72.006324
668.617729	25.127525	72.011329
667.744560	25.378553	72.016334
666.507822	32.781841	72.021338
666.310741	25.829264	72.026343
666.355883	26.678340	72.031348
665.462955	17.434997	72.036353
665.648391	37.502767	72.041358
664.431845	30.370352	72.046362
663.790107	23.985302	72.051367
662.788426	32.833423	72.056372
662.116817	39.664197	72.061377
661.859190	20.896270	72.066382
660.557666	36.544323	72.071386
659.621396	33.853489	72.076391
659.534012	17.280275	72.081396
658.863036	24.410549	72.086401
658.584075	35.510470	72.091406
657.626750	10.497597	72.096410
656.472969	31.658522	72.101415
656.255255	22.705024	72.106420
655.672889	36.142886	72.111425
655.067325	30.488476	72.116430
654.127529	30.732773	72.121434
653.651391	25.004141	72.126439
653.138522	16.990163	72.131444
651.848090	30.753658	72.136449
651.240602	34.204438	72.141454
651.057101	25.202916	72.146458
650.571703	34.754106	72.151463
649.861705	27.108968	72.156468
648.784482	29.762542	72.161473
648.512154	28.378860	72.166478
647.777678	20.855889	72.171482
646.247409	45.525419	72.176487
646.100538	20.481235	72.181492
645.424418	31.806820	72.186497
645.415286	29.819855	72.191502
644.216298	35.810570	72.196506
643.366208	24.754887	72.201511
642.736526	10.119300	72.206516
642.512927	38.469295	72.211521
642.169103	29.557956	72.216526
641.008405	25.652411	72.221530
640.468167	18.502191	72.226535
640.230032	39.296546	72.231540
639.052856	18.472177	72.236545
638.433561	18.946121	72.241550
638.003649	28.316593	72.246554
636.773036	26.855303	72.251559
636.178186	24.821277	72.256564
635.724835	20.410444	72.261569
635.420507	40.433212	72.266574
634.006425	24.861298	72.271578
633.015102	36.839454	72.276583
633.243748	16.018274	72.281588
632.359471	27.285550	72.286593
632.416170	24.163791	72.291598
631.141200	9.870662	72.296602
630.340331	31.599830	72.301607
630.231588	20.304670	72.306612
629.119079	21.194617	72.311617
628.696954	24.973829	72.316622
627.929683	43.887673	72.321626
626.791202	18.832698	72.326631
626.450399	37.454699	72.331636
625.614233	37.520084	72.336641
625.314647	22.043483	72.341646
624.714359	45.580939	72.346650
623.863479	17.424177	72.351655
622.962077	35.011146	72.356660
622.871746	26.642886	72.361665
622.176878	22.180638	72.366670
621.151590	21.664318	72.371674
620.255824	24.575993	72.376679
619.998490	28.909252	72.381684
618.776692	29.133823	72.386689
618.178887	23.069781	72.391694
617.457236	24.717458	72.396698
617.015336	47.422332	72.401703
617.054506	10.460476	72.406708
616.211553	34.456010	72.411713
615.118945	23.856838	72.416718
614.719207	24.593849	72.421722
614.056981	29.896720	72.426727
613.232009	6.956893	72.431732
612.299091	39.127081	72.436737
612.303170	23.289897	72.441742
611.663077	23.421825	72.446746
610.624755	31.682892	72.451751
609.958468	20.985864	72.456756
609.020040	35.658363	72.461761
608.912615	37.182987	72.466766
608.063559	16.278000	72.471770
607.065232	35.460437	72.476775
606.872194	31.145335	72.481780
606.051747	26.064458	72.486785
605.205105	28.641903	72.491790
604.441008	30.624334	72.496794
603.807059	6.715849	72.501799
603.797340	29.038062	72.506804
602.134036	35.443350	72.511809
602.213265	5.561611	72.516814
601.644373	42.066993	72.521818
601.005579	15.659918	72.526823
600.407470	26.198836	72.531828
599.219981	15.376682	72.536833
598.826495	30.126378	72.541838
597.865235	41.309745	72.546842
597.312098	26.860655	72.551847
597.085163	29.563316	72.556852
596.756094	31.747683	72.561857
595.651275	32.499233	72.566862
595.062692	22.478928	72.571866
593.966867	47.823568	72.576871
592.924897	23.620520	72.581876
592.369026	24.434439	72.586881
592.194328	41.653376	72.591886
591.669163	9.502583	72.596890
590.720795	39.428190	72.601895
590.344803	7.994774	72.606900
589.350121	30.478597	72.611905
589.312469	17.494329	72.616910
588.657234	34.573763	72.621914
587.564176	29.927378	72.626919
587.114639	26.151427	72.631924
585.719744	35.270350	72.636929
584.935157	3.164050	72.641934
584.271849	26.345677	72.646938
583.864420	31.483398	72.651943
584.245072	26.660629	72.656948
583.480370	30.973783	72.661953
582.466944	30.184367	72.666958
581.977767	11.335093	72.671962
580.814914	27.505097	72.676967
579.938090	29.234268	72.681972
579.235107	27.550201	72.686977
579.439846	18.177789	72.691982
578.241928	27.137610	72.696986
577.398790	23.440124	72.701991
576.935203	17.592827	72.706996
576.543136	31.522324	72.712001
575.547674	19.611513	72.717006
574.809012	14.115523	72.722010
573.955619	16.132684	72.727015
574.039710	15.826012	72.732020
573.001475	25.630833	72.737025
571.984525	32.764197	72.742030
571.618647	20.587533	72.747034
570.784790	17.675433	72.752039
570.778538	21.191300	72.757044
569.261800	30.376941	72.762049
568.920417	20.522266	72.767054
568.314995	21.413466	72.772058
568.141152	29.987833	72.777063
567.134231	24.446266	72.782068
566.341570	31.846666	72.787073
565.787241	25.564414	72.792078
565.329691	27.881208	72.797082
563.869330	23.193999	72.802087
563.715001	16.994685	72.807092
563.275316	21.820591	72.812097
562.539746	25.294943	72.817102
561.453775	25.020114	72.822106
560.884201	28.316645	72.827111
560.617180	16.699800	72.832116
560.013484	22.423842	72.837121
559.135220	24.077559	72.842126
558.479993	21.654223	72.847130
557.677904	22.474255	72.852135
557.775433	17.806966	72.857140
556.540112	19.672093	72.862145
556.016590	25.906888	72.867150
555.372936	28.146100	72.872154
554.113178	27.651388	72.877159
553.727182	27.553630	72.882164
552.981296	25.795985	72.887169
552.635819	23.441576	72.892174
551.672614	25.753767	72.897178
550.919824	17.227707	72.902183
550.599934	19.227699	72.907188
550.085726	24.934335	72.912193
549.351147	19.626927	72.917198
548.433207	21.141895	72.922202
547.765838	22.413532	72.927207
547.276907	18.170806	72.932212
545.936055	28.566286	72.937217
545.545854	21.327541	72.942222
545.405418	15.051904	72.947226
544.680851	29.102170	72.952231
544.738367	23.457284	72.957236
542.829657	24.649133	72.962241
542.405795	20.385004	72.967246
542.274069	12.002857	72.972250
541.551202	18.576896	72.977255
540.847925	22.574360	72.982260
539.778619	17.025401	72.987265
539.324535	15.456233	72.992270
537.980012	20.449932	72.997274
537.399795	30.169191	73.002279
537.261282	14.835690	73.007284
536.416051	22.093087	73.012289
536.612284	14.425056	73.017294
535.551739	21.519643	73.022298
534.811989	20.473773	73.027303
534.398388	15.482651	73.032308
533.230071	30.701112	73.037313
532.536217	22.950951	73.042318
532.002951	13.298736	73.047322
531.268212	15.773224	73.052327
531.165743	9.884185	73.057332
529.868857	24.113923	73.062337
529.229272	22.842374	73.067342
528.884417	19.639513	73.072346
528.320549	21.889674	73.077351
527.208824	14.256547	73.082356
526.540275	19.942042	73.087361
526.278792	22.210262	73.092366
525.209444	20.598767	73.097370
524.198394	25.501507	73.102375
524.160919	17.209996	73.107380
523.704310	31.864098	73.112385
523.095747	30.434652	73.117390
522.162326	24.890859	73.122394
521.723451	21.305604	73.127399
521.175964	22.182855	73.132404
519.786869	32.177624	73.137409
519.249100	20.804179	73.142414
518.807239	14.369994	73.147418
518.224105	27.402725	73.152423
517.662230	24.239168	73.157428
516.645343	33.146523	73.162433
516.445403	17.322941	73.167438
515.765332	33.155876	73.172442
514.684902	27.526700	73.177447
514.116771	25.244035	73.182452
513.382083	22.866485	73.187457
513.104055	24.380443	73.192462
512.189935	29.106905	73.197466
511.399826	28.206253	73.202471
511.174956	11.990855	73.207476
510.020533	24.937986	73.212481
508.994047	23.847921	73.217486
508.668601	19.640657	73.222490
508.310050	20.028942	73.227495
508.341904	16.300895	73.232500
507.223215	29.324335	73.237505
506.691315	22.683731	73.242510
505.675210	26.838269	73.247514
504.583642	36.978027	73.252519
504.361157	18.398510	73.257524
503.522726	23.056148	73.262529
503.177106	21.113334	73.267534
502.313707	26.670615	73.272538
501.520130	18.800743	73.277543
501.271284	29.086925	73.282548
500.450382	28.148606	73.287553
499.655807	9.493094	73.292558
498.879530	40.698517	73.297562
498.294460	18.622493	73.302567
497.817790	26.863497	73.307572
496.369699	33.031146	73.312577
495.793838	21.646431	73.317582
495.678482	27.936051	73.322586
495.557391	26.909898	73.327591
495.304752	18.334139	73.332596
493.771406	26.891714	73.337601
493.276288	23.704913	73.342606
492.266995	17.693854	73.347610
491.326006	31.333931	73.352615
491.242358	14.212988	73.357620
490.254120	20.651130	73.362625
489.660166	23.175737	73.367630
488.828631	29.838065	73.372634
488.250708	25.320961	73.377639
488.092497	28.834229	73.382644
487.371242	32.177018	73.387649
486.341782	21.083759	73.392654
486.052554	16.260480	73.397658
485.293587	22.586408	73.402663
484.441610	27.019142	73.407668
483.325051	22.343440	73.412673
483.093026	15.812758	73.417678
482.613131	25.328389	73.422682
482.067145	22.942861	73.427687
481.284578	14.580839	73.432692
480.176956	29.646150	73.437697
479.992590	28.478698	73.442702
479.328562	20.283859	73.447706
478.286269	18.880952	73.452711
477.517471	22.931446	73.457716
477.252656	23.008350	73.462721
476.865169	24.276413	73.467726
475.598827	18.878719	73.472730
475.141856	23.248521	73.477735
475.223859	18.624705	73.482740
474.307557	8.584130	73.487745
473.411104	10.336961	73.492750
472.910094	12.499851	73.497754
471.517161	19.221661	73.502759
470.983820	17.444372	73.507764
470.254033	15.389314	73.512769
470.222625	1.623534	73.517774
469.766794	0.601833	73.522778
468.317033	15.917175	73.527783
467.859694	3.646323	73.532788
467.453005	10.660405	73.537793
466.762547	13.061627	73.542798
465.736353	10.804652	73.547802
464.789437	11.548445	73.552807
464.971934	8.532798	73.557812
464.135624	16.507842	73.562817
463.630312	16.626218	73.567822
462.397546	18.405831	73.572826
462.002267	16.773695	73.577831
461.526499	13.993807	73.582836
460.480248	12.645153	73.587841
459.959321	10.591513	73.592846
459.466329	21.610411	73.597850
458.906480	25.602389	73.602855
458.038778	12.263145	73.607860
457.180390	21.749199	73.612865
456.893323	13.748187	73.617870
455.906530	17.150634	73.622874
454.870590	18.709666	73.627879
454.802778	12.102366	73.632884
454.162710	19.497396	73.637889
453.638302	16.600686	73.642894
452.845282	24.332309	73.647898
452.089699	19.660607	73.652903
451.753695	21.816134	73.657908
450.460293	17.162319	73.662913
449.613873	18.435703	73.667918
449.371616	21.345806	73.672922
448.921818	18.675317	73.677927
448.546596	16.256282	73.682932
447.239835	23.275020	73.687937
447.019083	19.456342	73.692942
446.328226	7.850294	73.697946
445.470594	16.306532	73.702951
444.912325	6.915363	73.707956
443.803159	13.699197	73.712961
443.470816	12.801320	73.717966
443.249734	18.108045	73.722970
442.467514	21.876850	73.727975
442.051667	12.111343	73.732980
440.548189	15.730155	73.737985
439.732523	11.120070	73.742990
439.077528	17.855196	73.747994
438.270961	11.780326	73.752999
438.395881	18.408527	73.758004
437.877200	16.775559	73.763009
437.663885	14.020086	73.768014
436.663549	19.696968	73.773018
435.784994	15.639347	73.778023
434.666434	14.617600	73.783028
433.894305	21.636306	73.788033
433.338538	28.221592	73.793038
433.270005	16.569996	73.798042
432.632716	18.678919	73.803047
432.358848	12.916542	73.808052
431.248812	21.176473	73.813057
430.031434	19.788871	73.818062
429.604826	16.542287	73.823066
428.720625	21.109473	73.828071
428.402646	19.427180	73.833076
427.490576	13.312358	73.838081
426.730805	17.668915	73.843086
426.044574	21.368816	73.848090
425.794937	21.987327	73.853095
425.593584	20.828895	73.858100
424.853145	18.062803	73.863105
423.958474	18.850324	73.868110
422.878014	9.479293	73.873114
421.823035	20.586165	73.878119
421.459279	15.680162	73.883124
421.036632	22.472881	73.888129
420.666958	22.844028	73.893134
419.766466	27.573079	73.898138
418.558742	27.715085	73.903143
418.771548	20.523780	73.908148
418.175071	27.355239	73.913153
417.140017	23.095492	73.918158
416.638347	13.044062	73.923162
415.766659	19.703340	73.928167
415.105216	16.697595	73.933172
414.027295	31.892228	73.938177
413.866203	22.674300	73.943182
413.523532	16.618553	73.948186
412.574320	18.942756	73.953191
411.958196	16.207320	73.958196
410.946992	32.490401	73.963201
410.585698	15.285991	73.968206
409.649993	15.635378	73.973210
408.731078	12.705355	73.978215
408.479174	0.810197	73.983220
407.854134	18.996507	73.988225
407.713722	10.450193	73.993230
406.540228	17.960193	73.998234
405.783565	21.478943	74.003239
405.439315	19.078634	74.008244
404.385155	8.233780	74.013249
403.643606	14.713059	74.018254
403.217158	6.431513	74.023258
402.553796	24.885697	74.028263
401.851358	18.877820	74.033268
400.763658	14.599665	74.038273
400.336112	19.070437	74.043278
400.073994	7.911725	74.048282
399.341080	22.259785	74.053287
399.120171	1.574949	74.058292
397.962129	16.548961	74.063297
397.618314	17.210865	74.068302
396.897985	12.511491	74.073306
395.351100	21.153269	74.078311
394.999459	12.766766	74.083316
394.672696	17.133173	74.088321
394.067483	17.679046	74.093326
393.358748	6.515817	74.098330
392.532202	11.450695	74.103335
392.319971	8.393874	74.108340
391.688475	26.631682	74.113345
390.800278	10.569330	74.118350
390.421066	11.985888	74.123354
389.172875	34.475455	74.128359
388.718105	8.892272	74.133364
387.710071	21.868148	74.138369
386.890511	29.804281	74.143374
387.211149	17.869912	74.148378
385.781993	25.469548	74.153383
385.186489	21.207576	74.158388
384.731177	22.303544	74.163393
384.207711	8.554687	74.168398
383.698418	20.087093	74.173402
382.412440	18.726215	74.178407
382.193473	28.362693	74.183412
381.749555	14.668960	74.188417
380.796144	34.774633	74.193422
380.491087	13.686901	74.198426
379.503351	26.760468	74.203431
379.006467	20.748224	74.208436
377.782255	10.758340	74.213441
377.392082	25.149552	74.218446
376.708255	25.592846	74.223450
375.573927	30.766008	74.228455
375.365620	11.963517	74.233460
374.434657	47.334459	74.238465
374.190787	14.757348	74.243470
373.804583	12.076741	74.248474
373.005950	14.269734	74.253479
372.569540	12.623670	74.258484
371.589013	17.322911	74.263489
371.304961	18.572929	74.268494
370.262603	14.864697	74.273498
369.304927	28.023359	74.278503
369.407340	21.904573	74.283508
367.852168	28.824172	74.288513
367.092632	21.038811	74.293518
366.570394	12.919186	74.298522
366.066479	25.015259	74.303527
366.056038	21.355452	74.308532
364.986692	20.467812	74.313537
364.214057	16.563642	74.318542
363.478409	11.980256	74.323546
363.108558	20.243669	74.328551
362.019224	15.234126	74.333556
361.374120	29.702239	74.338561
360.979677	22.342795	74.343566
360.722492	17.361474	74.348570
359.468118	23.807383	74.353575
359.168105	19.758510	74.358580
358.580432	21.034841	74.363585
357.707165	20.823969	74.368590
356.714480	24.429232	74.373594
355.888671	19.983210	74.378599
356.186624	5.406481	74.383604
355.180169	15.133761	74.388609
354.325515	3.974883	74.393614
353.728671	16.719660	74.398618
352.871644	20.240228	74.403623
352.540162	11.003745	74.408628
351.866090	19.003422	74.413633
350.922026	19.117633	74.418638
350.627332	11.958331	74.423642
349.565965	6.550123	74.428647
349.297225	8.040539	74.433652
348.634013	14.370157	74.438657
347.845284	20.235684	74.443662
347.278533	23.098166	74.448666
346.290538	22.177070	74.453671
345.944055	13.556380	74.458676
344.817165	18.927050	74.463681
343.887260	18.573831	74.468686
343.462237	19.497830	74.473690
343.130414	26.804335	74.478695
343.048668	21.722520	74.483700
342.210518	17.655343	74.488705
341.174975	18.728682	74.493710
340.996543	10.095403	74.498714
339.482052	24.755686	74.503719
338.986243	25.954306	74.508724
338.365806	22.894741	74.513729
337.817856	21.930322	74.518734
336.798146	16.285255	74.523738
335.962041	21.477128	74.528743
335.852409	10.689919	74.533748
335.453118	13.251338	74.538753
335.012390	12.186257	74.543758
333.984849	4.911963	74.548762
332.847083	19.537432	74.553767
332.958385	19.585942	74.558772
331.518727	21.848000	74.563777
330.767952	18.323537	74.568782
330.310506	21.706314	74.573786
329.693418	27.162889	74.578791
329.623881	18.352987	74.583796
329.084806	26.132471	74.588801
328.240021	16.265056	74.593806
327.739116	11.721535	74.598810
326.361606	10.908259	74.603815
325.503631	11.215328	74.608820
324.878743	24.833440	74.613825
324.535960	22.989544	74.618830
324.314821	16.381464	74.623834
323.262591	22.046157	74.628839
322.953507	6.042925	74.633844
322.391014	12.452684	74.638849
321.433626	8.478635	74.643854
320.841639	11.627402	74.648858
320.037832	13.535822	74.653863
319.355190	11.405494	74.658868
318.230671	9.837578	74.663873
317.887500	23.365058	74.668878
317.574132	11.411904	74.673882
317.011949	19.846316	74.678887
316.379033	16.176923	74.683892
315.444527	15.720375	74.688897
314.621703	15.750624	74.693902
313.716879	18.296433	74.698906
312.687342	13.067662	74.703911
312.575697	7.820317	74.708916
311.949688	8.473597	74.713921
311.277922	26.817172	74.718926
311.490744	9.508679	74.723930
309.867377	7.660753	74.728935
309.449803	24.516245	74.733940
308.757529	-2.284213	74.738945
307.951949	24.554767	74.743950
307.680484	15.546833	74.748954
306.982705	15.544539	74.753959
306.384525	15.878011	74.758964
305.467397	-3.423285	74.763969
304.734235	15.775262	74.768974
304.137184	15.643379	74.773978
303.596165	14.228456	74.778983
302.946138	10.762058	74.783988
302.167759	17.341843	74.788993
301.311970	14.575257	74.793998
301.414251	2.432868	74.799002
299.950689	30.367009	74.804007
299.570011	15.956784	74.809012
298.768806	3.053283	74.814017
298.012994	16.052049	74.819022
297.570373	18.044824	74.824026
296.847231	20.897553	74.829031
296.470321	8.169255	74.834036
295.828214	23.493129	74.839041
294.554734	22.936087	74.844046
294.138021	9.051981	74.849050
293.682477	19.579246	74.854055
292.991647	15.307267	74.859060
291.886316	28.038499	74.864065
291.086987	16.054005	74.869070
291.076435	17.490658	74.874074
290.599858	25.477793	74.879079
289.702565	15.632957	74.884084
288.888840	21.791050	74.889089
288.359959	18.062507	74.894094
288.046173	19.146970	74.899098
286.941109	25.389349	74.904103
286.395458	5.281404	74.909108
285.698728	17.384557	74.914113
284.850148	17.381077	74.919118
284.397273	20.223843	74.924122
283.430133	21.611137	74.929127
283.036194	11.384891	74.934132
282.469990	19.985520	74.939137
281.364547	12.121302	74.944142
280.862115	4.015896	74.949146
280.266091	19.702986	74.954151
280.125147	15.863725	74.959156
279.358989	16.424242	74.964161
278.451230	11.489872	74.969166
278.267383	1.357872	74.974170
276.492566	21.849930	74.979175
276.080551	9.540373	74.984180
275.678819	14.844360	74.989185
275.243118	19.988193	74.994190
274.728370	24.431884	74.999194
273.473227	19.756304	75.004199
273.272832	21.186951	75.009204
272.853537	15.006260	75.014209
271.779561	21.049733	75.019214
271.387063	22.216127	75.024218
270.402413	23.235654	75.029223
269.563595	17.194373	75.034228
268.833310	21.268744	75.039233
268.127503	16.532407	75.044238
267.795765	11.700175	75.049242
267.442312	12.727889	75.054247
266.946742	9.057118	75.059252
266.038831	22.920612	75.064257
265.453839	19.535315	75.069262
264.535541	8.588460	75.074266
263.456170	19.221477	75.079271
263.388117	13.137755	75.084276
262.716814	2.875314	75.089281
261.914079	14.758837	75.094286
261.226612	21.625324	75.099290
260.609616	13.908745	75.104295
260.068838	13.629138	75.109300
259.030459	17.519247	75.114305
258.132273	22.875572	75.119310
257.898793	16.701532	75.124314
257.196465	10.469776	75.129319
256.803951	24.017737	75.134324
256.006796	21.355354	75.139329
255.481449	14.931390	75.144334
255.052489	13.649995	75.149338
253.591801	19.564319	75.154343
253.119638	13.693243	75.159348
252.772795	24.430254	75.164353
252.166329	20.485442	75.169358
251.194988	13.847164	75.174362
250.612799	21.062703	75.179367
250.428012	16.104550	75.184372
249.173454	14.581050	75.189377
248.342101	17.100977	75.194382
248.021591	10.081422	75.199386
247.650167	12.608449	75.204391
246.967642	19.472573	75.209396
245.989614	13.193313	75.214401
245.225828	16.604437	75.219406
245.021098	5.004553	75.224410
243.729238	21.978916	75.229415
243.482944	14.367241	75.234420
242.611925	15.591002	75.239425
242.021383	8.482039	75.244430
241.288148	12.340854	75.249434
240.126487	18.901337	75.254439
239.512110	2.451667	75.259444
239.132472	24.834331	75.264449
239.120276	21.395572	75.269454
238.981931	7.541222	75.274458
237.789858	15.970407	75.279463
237.000534	10.220858	75.284468
235.983163	20.651623	75.289473
234.895673	20.588481	75.294478
234.941434	16.588580	75.299482
234.419997	16.659113	75.304487
233.800662	16.365229	75.309492
232.769959	13.853623	75.314497
232.160856	17.730497	75.319502
231.564902	12.748015	75.324506
230.260817	22.639475	75.329511
229.887152	22.492496	75.334516
229.055738	19.144918	75.339521
228.810598	13.512030	75.344526
228.670525	13.354620	75.349530
227.702334	20.641160	75.354535
227.010162	16.471913	75.359540
226.699204	18.407440	75.364545
225.501650	21.791535	75.369550
224.333719	22.088133	75.374554
224.024774	16.068047	75.379559
223.578770	13.732874	75.384564
223.407902	11.090502	75.389569
222.461586	17.239788	75.394574
221.750456	23.405196	75.399578
220.903494	22.803848	75.404583
220.055004	11.008568	75.409588
219.287801	19.825742	75.414593
218.765537	12.641248	75.419598
218.670098	8.769511	75.424602
217.818160	15.736337	75.429607
217.092259	14.830277	75.434612
216.457433	17.243193	75.439617
215.389505	22.191377	75.444622
214.731092	14.891402	75.449626
213.960273	25.547784	75.454631
213.750829	18.707633	75.459636
213.193981	14.808537	75.464641
212.658054	18.533408	75.469646
211.769951	14.005917	75.474650
210.921971	33.475099	75.479655
210.587943	27.418011	75.484660
209.438468	18.382928	75.489665
208.416949	24.361295	75.494670
208.240546	19.078553	75.499674
207.719825	21.910072	75.504679
207.527888	27.877599	75.509684
206.546621	20.808859	75.514689
205.475354	26.022495	75.519694
205.164633	19.075496	75.524698
204.214029	22.090664	75.529703
203.700694	13.755215	75.534708
203.527276	15.017571	75.539713
202.714772	28.728685	75.544718
202.148843	11.631088	75.549722
201.138215	25.766427	75.554727
200.375541	18.058901	75.559732
199.460486	18.865520	75.564737
198.521853	14.863303	75.569742
198.474324	10.908238	75.574746
197.930845	20.022467	75.579751
197.586638	9.782009	75.584756
196.512600	11.933813	75.589761
195.448312	15.296672	75.594766
195.248957	4.274652	75.599770
194.612119	16.037127	75.604775
194.037901	11.552635	75.609780
193.232344	24.655547	75.614785
192.595978	25.890795	75.619790
192.149699	10.620639	75.624794
191.206959	30.119119	75.629799
190.567231	19.263489	75.634804
190.163696	11.721048	75.639809
189.248589	12.713749	75.644814
188.497769	11.720213	75.649818
187.664744	22.268250	75.654823
187.310058	20.576077	75.659828
186.509103	15.711444	75.664833
185.783059	11.599649	75.669838
185.761399	5.309855	75.674842
184.731065	18.781320	75.679847
183.979347	17.959806	75.684852
183.328190	18.333292	75.689857
182.787341	23.556977	75.694862
181.937399	6.968277	75.699866
181.253874	23.232269	75.704871
180.674309	17.110267	75.709876
180.302850	17.521155	75.714881
179.008397	18.498654	75.719886
178.444797	0.486128	75.724890
177.771797	18.028850	75.729895
177.546450	12.034867	75.734900
176.845273	16.998701	75.739905
175.773216	15.178074	75.744910
175.553666	11.461738	75.749914
174.809140	20.704214	75.754919
174.028521	21.995581	75.759924
173.212753	17.589029	75.764929
172.870247	18.383211	75.769934
172.254662	23.902650	75.774938
170.794154	21.109536	75.779943
170.309181	21.590562	75.784948
170.234653	19.252936	75.789953
169.474975	31.847100	75.794958
169.146222	24.100356	75.799962
167.755225	19.216275	75.804967
167.009408	15.743115	75.809972
166.803331	19.886883	75.814977
166.361198	24.263823	75.819982
165.973273	10.379898	75.824986
164.747525	18.016590	75.829991
164.271910	12.950289	75.834996
163.428377	11.400718	75.840001
162.429323	21.957889	75.845006
162.062201	12.190998	75.850010
161.744947	16.529102	75.855015
161.158022	18.005619	75.860020
159.984019	19.772855	75.865025
159.403624	21.193141	75.870030
158.960447	14.907482	75.875034
157.794479	18.040579	75.880039
157.018530	13.637146	75.885044
156.463980	21.360774	75.890049
155.999890	18.528631	75.895054
155.884087	13.649374	75.900058
155.333067	23.400289	75.905063
154.395404	11.038972	75.910068
153.751579	12.808399	75.915073
153.164118	18.835837	75.920078
152.207839	24.879510	75.925082
151.469163	18.089067	75.930087
150.992885	12.873073	75.935092
149.956779	14.623055	75.940097
149.104653	22.547090	75.945102
148.787103	10.187817	75.950106
148.389337	23.575775	75.955111
148.049661	18.952976	75.960116
147.230262	21.521488	75.965121
146.621757	20.178861	75.970126
145.998898	14.800170	75.975130
144.569786	17.688244	75.980135
143.934451	18.946993	75.985140
143.634921	16.145380	75.990145
143.232365	15.938371	75.995150
142.551906	15.576991	76.000154
141.956371	17.948968	76.005159
141.159617	20.649482	76.010164
140.109027	13.762133	76.015169
139.440676	18.413254	76.020174
139.063724	17.498881	76.025178
138.310697	14.145145	76.030183
137.861774	14.219905	76.035188
136.850018	9.932925	76.040193
136.003808	24.986604	76.045198
135.821452	12.910109	76.050202
135.358401	8.616054	76.055207
134.421709	18.333855	76.060212
133.759741	23.179492	76.065217
133.201544	14.474346	76.070222
132.847828	13.993061	76.075226
131.724705	16.412902	76.080231
131.016185	18.137461	76.085236
130.503621	22.580826	76.090241
129.619320	19.277986	76.095246
128.759123	2.795027	76.100250
128.035031	24.453638	76.105255
127.860841	14.756908	76.110260
127.355857	17.555971	76.115265
126.506653	28.642740	76.120270
125.974441	11.311154	76.125274
125.193777	15.565472	76.130279
124.625582	13.468989	76.135284
123.791405	7.953704	76.140289
122.753518	12.728406	76.145294
122.553617	19.895617	76.150298
122.041037	24.413100	76.155303
121.439732	17.250698	76.160308
120.789291	17.010686	76.165313
119.958504	21.129504	76.170318
119.427298	12.137802	76.175322
118.455668	9.888048	76.180327
117.699252	19.217582	76.185332
117.573256	15.100002	76.190337
116.384635	21.190198	76.195342
115.494682	15.546621	76.200346
114.927875	15.094589	76.205351
114.720151	12.033928	76.210356
114.275697	11.598653	76.215361
112.801015	16.529742	76.220366
112.586958	7.107445	76.225370
112.151305	19.131147	76.230375
111.571660	9.915374	76.235380
110.830765	3.153691	76.240385
110.024365	12.161627	76.245390
109.605245	16.336217	76.250394
108.654154	19.911283	76.255399
107.705816	11.957454	76.260404
107.475654	8.534540	76.265409
106.346998	15.985470	76.270414
105.764442	5.079768	76.275418
105.166269	17.840552	76.280423
104.481133	15.045249	76.285428
104.209557	6.857351	76.290433
103.530842	20.121386	76.295438
102.859297	6.566550	76.300442
101.829689	15.007725	76.305447
101.924931	10.858020	76.310452
100.996340	17.255240	76.315457
99.974032	25.706295	76.320462
99.785573	0.858187	76.325466
98.665372	20.151594	76.330471
98.019478	18.103776	76.335476
97.778342	10.464502	76.340481
96.618079	19.281311	76.345486
95.885234	-2.002987	76.350490
95.193563	27.274590	76.355495
94.906628	14.151974	76.360500
94.545466	-4.353239	76.365505
93.363932	17.094478	76.370510
93.063771	12.969986	76.375514
92.198439	5.863898	76.380519
91.339306	20.061826	76.385524
90.330236	12.251724	76.390529
89.729184	17.204342	76.395534
89.512896	11.223120	76.400538
88.933411	21.557290	76.405543
88.248160	19.064768	76.410548
87.515051	17.893407	76.415553
86.587241	19.580415	76.420558
86.207515	24.329014	76.425562
85.674990	19.998741	76.430567
84.816466	13.698921	76.435572
84.275621	17.074535	76.440577
83.874188	20.352226	76.445582
82.954048	4.318796	76.450586
82.117348	14.079005	76.455591
81.875377	17.570949	76.460596
81.275679	16.848219	76.465601
79.841475	7.655211	76.470606
79.702475	6.113152	76.475610
78.789300	13.941287	76.480615
78.282862	9.409751	76.485620
77.440239	23.280219	76.490625
76.627139	21.883512	76.495630
76.355339	3.077055	76.500634
75.704843	26.581478	76.505639
74.741650	15.723869	76.510644
74.293510	6.351528	76.515649
73.510537	14.570461	76.520654
73.440008	14.851374	76.525658
72.361682	21.359213	76.530663
71.332101	14.164213	76.535668
70.953262	1.680710	76.540673
70.631223	19.736716	76.545678
69.991357	8.766052	76.550682
69.038590	18.997338	76.555687
68.370642	13.766205	76.560692
67.312482	13.102406	76.565697
66.132855	18.528905	76.570702
66.123126	12.607778	76.575706
65.617982	14.782439	76.580711
65.311104	16.023512	76.585716
64.614022	21.827190	76.590721
63.467430	20.193532	76.595726
63.295911	9.039370	76.600730
62.967013	20.333307	76.605735
61.977851	14.603080	76.610740
61.280857	11.708764	76.615745
60.211905	10.300833	76.620750
60.128374	19.247108	76.625754
58.916284	19.959235	76.630759
58.535123	9.820896	76.635764
58.403175	14.810658	76.640769
57.103741	21.479916	76.645774
56.608622	12.200219	76.650778
55.638386	22.047966	76.655783
54.845386	3.903352	76.660788
53.853763	8.131412	76.665793
53.272621	27.349901	76.670798
53.287232	17.686145	76.675802
52.789549	17.223103	76.680807
52.237549	11.929331	76.685812
51.754266	16.651872	76.690817
50.424078	23.384383	76.695822
49.958824	13.071809	76.700826
48.676758	24.232363	76.705831
48.115085	16.440803	76.710836
48.093597	17.295758	76.715841
47.793132	15.017828	76.720846
46.691221	6.039912	76.725850
45.935514	13.691562	76.730855
45.836617	10.345485	76.735860
44.829889	13.021173	76.740865
43.612592	26.746417	76.745870
43.335268	10.284064	76.750874
42.314771	17.899107	76.755879
41.376015	7.206349	76.760884
41.047482	10.666371	76.765889
40.394711	15.789663	76.770894
40.035799	17.426947	76.775898
39.824514	10.126679	76.780903
38.858359	9.071348	76.785908
38.332721	11.780684	76.790913
37.152173	12.863084	76.795918
36.400771	12.848921	76.800922
35.768990	10.745258	76.805927
35.294535	7.091675	76.810932
34.963658	11.673221	76.815937
34.047639	12.011726	76.820942
33.188451	8.462084	76.825946
32.657654	10.432696	76.830951
32.191824	2.318374	76.835956
31.517200	8.717679	76.840961
30.363682	11.883536	76.845966
30.271392	7.134577	76.850970
29.744542	17.867186	76.855975
28.869750	17.144195	76.860980
28.060798	11.150289	76.865985
27.347803	13.143656	76.870990
26.529072	-0.105405	76.875994
25.354653	20.073403	76.880999
25.006440	17.831476	76.886004
25.141788	6.817599	76.891009
24.690010	4.445546	76.896014
24.073737	7.150419	76.901018
22.767187	4.260309	76.906023
22.201848	9.557304	76.911028
21.172206	15.327306	76.916033
20.073510	18.996905	76.921038
20.008633	-7.644842	76.926042
19.591221	7.873421	76.931047
18.983205	1.784398	76.936052
18.214294	12.508309	76.941057
17.542043	14.193999	76.946062
17.370002	10.060122	76.951066
16.441224	17.649506	76.956071
15.356892	16.792797	76.961076
14.835238	19.742764	76.966081
14.375110	4.312469	76.971086
13.619576	2.170209	76.976090
12.710837	18.695628	76.981095
12.077096	24.643747	76.986100
11.903516	5.676568	76.991105
10.351691	16.373988	76.996110
10.098354	-1.970211	77.001114
9.393447	10.000248	77.006119
9.169562	3.466776	77.011124
8.750394	8.201170	77.016129
7.305451	14.040576	77.021134
6.990459	15.514749	77.026139
6.561924	3.785046	77.031143
5.607759	13.150873	77.036148
4.852544	10.603310	77.041153
4.241155	17.090303	77.046158