Mon Mar 08 18:51:35 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.002629	109.486449	0.000000
-0.773298	93.362646	0.005005
-1.761595	63.490423	0.010010
-3.340059	15.078619	0.015014
-7.380614	-17.543868	0.020019
-13.062002	-18.529844	0.025024
-17.753595	-18.618776	0.030029
-22.613173	-10.481243	0.035034
-26.684559	-8.970814	0.040038
-30.315026	-16.668603	0.045043
-34.113437	-10.149456	0.050048
-37.524395	-12.841037	0.055053
-40.974067	-4.570430	0.060058
-44.834072	-17.086725	0.065062
-48.555298	-12.819007	0.070067
-52.427814	-19.527301	0.075072
-55.979535	-10.552888	0.080077
-60.154782	-3.377531	0.085082
-63.635045	-6.707685	0.090086
-67.378812	-23.876863	0.095091
-71.359788	0.948817	0.100096
-74.848949	-17.870947	0.105101
-79.006075	-12.712099	0.110106
-82.714780	-19.802846	0.115110
-86.264199	-9.385935	0.120115
-90.218620	-1.853121	0.125120
-93.753118	-12.506963	0.130125
-97.351786	-3.020405	0.135130
-101.262316	-13.667852	0.140134
-105.071990	-9.009069	0.145139
-109.322448	4.190929	0.150144
-112.573547	-7.271303	0.155149
-116.326471	-8.421235	0.160154
-119.717147	-12.828400	0.165158
-123.569733	-9.741174	0.170163
-127.693766	-18.039681	0.175168
-131.481775	-24.193657	0.180173
-135.508129	-15.884527	0.185178
-139.468602	-9.162755	0.190182
-143.260596	-13.658805	0.195187
-147.336197	-7.382245	0.200192
-150.499068	-19.954404	0.205197
-154.282088	-9.372400	0.210202
-158.050996	-8.979128	0.215206
-161.312027	-12.110745	0.220211
-165.314233	0.223453	0.225216
-169.070941	-14.929848	0.230221
-172.797423	-12.003009	0.235226
-176.593003	-9.583922	0.240230
-180.338541	-15.435536	0.245235
-184.395298	-5.312820	0.250240
-187.863733	-1.905197	0.255245
-191.790552	-8.222999	0.260250
-195.556045	-24.820817	0.265254
-199.233855	-17.309909	0.270259
-203.095502	-7.932617	0.275264
-206.467273	-14.261705	0.280269
-210.120038	-9.932135	0.285274
-214.432968	-14.441120	0.290278
-217.757684	-15.679730	0.295283
-221.971843	-16.361670	0.300288
-225.615516	-21.469422	0.305293
-229.511900	-18.274123	0.310298
-233.322142	0.313303	0.315302
-236.869397	-16.915335	0.320307
-240.610167	-12.644211	0.325312
-244.372241	-18.786375	0.330317
-248.144932	-11.126217	0.335322
-252.081655	-5.776767	0.340326
-255.404809	-17.706643	0.345331
-259.447521	-5.704865	0.350336
-263.142189	-7.849398	0.355341
-267.126821	-10.021754	0.360346
-270.627737	-11.571191	0.365350
-274.537065	-12.410498	0.370355
-278.483318	-9.763789	0.375360
-282.162300	-9.140265	0.380365
-285.722672	-2.002762	0.385370
-289.341603	-8.812640	0.390374
-293.085535	-14.579177	0.395379
-296.992039	-7.646590	0.400384
-300.961283	-22.977025	0.405389
-304.664526	-7.874088	0.410394
-308.345456	-14.180481	0.415398
-311.845147	-13.437308	0.420403
-315.875180	-10.621057	0.425408
-319.512991	-15.685447	0.430413
-323.281254	-8.951495	0.435418
-327.425478	-11.240189	0.440422
-330.876987	-19.079602	0.445427
-334.745761	-7.616377	0.450432
-338.549059	-22.987427	0.455437
-342.425809	-13.771511	0.460442
-345.913946	-3.433409	0.465446
-349.582834	-17.625919	0.470451
-353.529957	-7.723856	0.475456
-357.343889	-13.477537	0.480461
-361.228632	-16.983929	0.485466
-364.954983	-11.954876	0.490470
-368.270724	-4.993502	0.495475
-372.153017	-5.594131	0.500480
-375.898043	-9.709397	0.505485
-379.978487	-4.529174	0.510490
-383.707257	-10.911382	0.515494
-386.916061	-16.015780	0.520499
-391.207049	-14.203192	0.525504
-394.690489	-6.527500	0.530509
-398.628878	-8.979814	0.535514
-402.485365	-14.263031	0.540518
-406.106100	-18.237253	0.545523
-410.249746	-5.113752	0.550528
-413.684930	-12.293371	0.555533
-417.858987	-8.973014	0.560538
-421.216899	-11.860156	0.565542
-424.549216	-13.040497	0.570547
-428.752398	-6.629573	0.575552
-432.486044	-14.471086	0.580557
-436.230168	-3.827075	0.585562
-440.083150	-15.148551	0.590566
-443.907263	-6.456512	0.595571
-447.848568	-4.638166	0.600576
-451.515981	-21.519266	0.605581
-455.223596	-5.445659	0.610586
-458.874795	-11.119511	0.615590
-462.245277	-21.442584	0.620595
-466.392004	-18.012978	0.625600
-469.997553	-17.802990	0.630605
-473.777302	-11.412309	0.635610
-477.890816	-18.625413	0.640614
-481.525537	-10.390892	0.645619
-485.279446	-9.635250	0.650624
-488.713931	-13.590207	0.655629
-492.534510	-8.049205	0.660634
-496.361204	-12.624288	0.665638
-499.949976	-24.330026	0.670643
-504.053296	-13.932887	0.675648
-507.648094	-22.290000	0.680653
-511.368143	-9.350684	0.685658
-515.502881	-16.779513	0.690662
-519.253640	-13.170225	0.695667
-523.223652	-14.426756	0.700672
-526.390662	-12.783991	0.705677
-530.261926	-14.261274	0.710682
-534.049476	-12.894672	0.715686
-537.588653	-16.277783	0.720691
-541.639090	-9.648233	0.725696
-544.998737	-14.742508	0.730701
-549.350092	-7.479867	0.735706
-553.220619	-1.687957	0.740710
-556.654769	-11.921880	0.745715
-560.802350	-8.652813	0.750720
-564.187258	-16.232867	0.755725
-567.959816	-12.843934	0.760730
-571.474962	-4.793952	0.765734
-575.187841	-15.774897	0.770739
-578.902605	-12.743662	0.775744
-582.787247	-9.849276	0.780749
-586.863561	-14.346487	0.785754
-590.823408	-22.921099	0.790758
-594.365482	-15.853895	0.795763
-598.087401	-8.458350	0.800768
-601.854385	-16.874535	0.805773
-605.536612	-13.116801	0.810778
-609.763547	-15.404398	0.815782
-613.168098	-9.557539	0.820787
-616.695789	-5.023436	0.825792
-620.405013	-12.209418	0.830797
-624.198301	-6.625267	0.835802
-628.107083	-5.343220	0.840806
-631.906250	-18.579364	0.845811
-635.641916	-10.662786	0.850816
-638.993329	-15.914345	0.855821
-642.833642	-16.361976	0.860826
-647.292070	-17.570223	0.865830
-651.057579	-6.471506	0.870835
-654.799201	-6.985346	0.875840
-658.118671	-14.705016	0.880845
-661.881278	-18.501638	0.885850
-665.740335	8.062001	0.890854
-669.500451	-18.693904	0.895859
-673.489431	-20.704036	0.900864
-676.982292	-22.465452	0.905869
-680.982525	-13.169369	0.910874
-684.391819	-16.763807	0.915878
-687.834284	-18.769786	0.920883
-692.119131	-3.582834	0.925888
-695.691296	-13.748757	0.930893
-699.892908	-24.220908	0.935898
-703.320893	-25.563749	0.940902
-706.994206	-7.662985	0.945907
-710.935431	-4.593781	0.950912
-714.323281	-24.813128	0.955917
-718.387261	-36.699582	0.960922
-722.276707	-4.187912	0.965926
-725.464363	-12.532480	0.970931
-730.097381	-13.165504	0.975936
-733.710559	-18.111756	0.980941
-737.164755	-10.064979	0.985946
-741.105128	-19.055573	0.990950
-744.252807	-23.823904	0.995955
-748.539490	-12.717446	1.000960
-752.078054	-16.486653	1.005965
-756.046743	-6.260420	1.010970
-759.862495	-17.800158	1.015974
-763.797303	-9.755373	1.020979
-767.550614	-9.450360	1.025984
-771.102081	-8.712432	1.030989
-774.859743	-18.556858	1.035994
-778.468490	-24.612266	1.040998
-782.118125	-2.702113	1.046003
-786.240930	-7.495873	1.051008
-789.623851	-23.571936	1.056013
-793.524935	-1.815528	1.061018
-797.647500	-10.065749	1.066022
-801.066076	-5.788502	1.071027
-805.242008	0.144078	1.076032
-808.594134	-6.953606	1.081037
-812.526309	-9.128690	1.086042
-816.239835	-3.511263	1.091046
-819.986663	-13.097168	1.096051
-823.776479	-6.138257	1.101056
-827.511344	-9.130124	1.106061
-831.264319	-5.236166	1.111066
-835.322815	-7.517167	1.116070
-838.656828	-6.714557	1.121075
-842.560039	-8.690808	1.126080
-845.887391	-14.034211	1.131085
-849.970585	-8.646202	1.136090
-853.836818	-1.526803	1.141094
-857.069088	-15.211124	1.146099
-861.570222	-19.447557	1.151104
-865.364092	-17.850777	1.156109
-869.192468	-5.227920	1.161114
-872.566654	-9.210867	1.166118
-876.019902	-15.111223	1.171123
-880.402961	-9.583766	1.176128
-883.588789	-3.651661	1.181133
-887.717003	-6.167411	1.186138
-891.594355	-2.370161	1.191142
-895.268874	-9.676347	1.196147
-898.997529	-11.541648	1.201152
-902.712867	-15.143598	1.206157
-906.659641	-9.001499	1.211162
-910.183093	-11.864618	1.216166
-913.773287	-6.028660	1.221171
-917.678326	-7.780580	1.226176
-921.463659	-12.892962	1.231181
-925.382229	-14.485020	1.236186
-928.948244	-9.304143	1.241190
-932.672302	-5.652754	1.246195
-936.392802	-23.057492	1.251200
-940.346617	-13.164488	1.256205
-944.059867	-1.020362	1.261210
-948.158777	-20.557963	1.266214
-951.824451	0.221232	1.271219
-955.224746	-11.969610	1.276224
-958.569556	-13.110926	1.281229
-962.404927	-3.845482	1.286234
-966.754417	-14.161031	1.291238
-970.420108	-15.665727	1.296243
-974.429393	-6.539600	1.301248
-978.106686	-15.690107	1.306253
-981.779728	-7.986437	1.311258
-985.754395	-4.499879	1.316262
-989.328030	-10.729292	1.321267
-993.130077	-10.354628	1.326272
-996.597471	-4.380502	1.331277
-1000.372194	-10.987717	1.336282
-1004.609096	-17.041649	1.341286
-1007.836993	-24.132084	1.346291
-1011.736869	-6.125289	1.351296
-1015.757253	-2.517837	1.356301
-1019.455285	-16.124264	1.361306
-1023.218003	-8.228007	1.366310
-1026.702086	-21.947476	1.371315
-1030.717666	10.405036	1.376320
-1034.212269	-11.394062	1.381325
-1037.809849	-21.826571	1.386330
-1042.027613	-13.573677	1.391334
-1045.568548	-6.059762	1.396339
-1049.453497	-12.537308	1.401344
-1053.155956	-2.100891	1.406349
-1056.987567	-13.599730	1.411354
-1060.940594	-13.719587	1.416358
-1064.117690	-5.535342	1.421363
-1068.099915	-2.436917	1.426368
-1071.805009	-11.499251	1.431373
-1075.820346	-23.548937	1.436378
-1079.473249	5.443720	1.441382
-1083.250060	-17.301975	1.446387
-1087.306238	-5.834444	1.451392
-1090.649099	-13.071942	1.456397
-1094.326119	-19.861767	1.461402
-1098.360981	-10.953686	1.466406
-1101.934540	-5.098036	1.471411
-1106.061081	-18.664145	1.476416
-1109.551367	-21.891779	1.481421
-1113.422093	-26.211215	1.486426
-1117.396563	-11.793834	1.491430
-1120.689827	-24.849862	1.496435
-1124.721400	-11.115565	1.501440
-1128.369964	-7.201580	1.506445
-1132.402991	-26.150150	1.511450
-1136.234377	2.197816	1.516454
-1139.643815	-22.538167	1.521459
-1143.656938	-11.509490	1.526464
-1146.978149	-21.282762	1.531469
-1150.786034	-3.547502	1.536474
-1154.876361	-0.218763	1.541478
-1157.982004	-13.993839	1.546483
-1162.305607	-6.966350	1.551488
-1166.051567	-25.210209	1.556493
-1169.923890	-24.436112	1.561498
-1174.063916	5.315794	1.566502
-1176.925459	-8.063108	1.571507
-1180.848686	-9.866861	1.576512
-1184.462853	-17.888644	1.581517
-1188.626795	-18.015535	1.586522
-1192.919279	-9.118112	1.591526
-1196.341851	-3.070455	1.596531
-1200.038169	-11.109031	1.601536
-1203.292640	-27.348461	1.606541
-1207.156452	-21.905077	1.611546
-1211.285840	-17.330601	1.616550
-1214.832675	-17.873135	1.621555
-1218.580028	-4.857472	1.626560
-1222.402792	-7.421498	1.631565
-1226.092199	-23.534532	1.636570
-1230.017484	-14.995406	1.641574
-1233.406809	-12.813114	1.646579
-1237.576507	-1.719803	1.651584
-1241.186551	-1.323425	1.656589
-1245.183299	-0.406298	1.661594
-1249.092352	-4.610573	1.666598
-1252.242125	-13.524943	1.671603
-1256.361519	-9.661562	1.676608
-1259.841194	-14.040178	1.681613
-1263.812866	-16.190824	1.686618
-1267.889355	3.415153	1.691622
-1271.361997	-14.769775	1.696627
-1275.060142	-3.272512	1.701632
-1278.636618	-15.639626	1.706637
-1282.638305	-24.830731	1.711642
-1286.737642	-1.242722	1.716646
-1290.006464	-3.192023	1.721651
-1293.935499	-5.324213	1.726656
-1297.266276	-12.689477	1.731661
-1301.043731	-15.850357	1.736666
-1305.379933	-6.437998	1.741670
-1308.860476	-21.972504	1.746675
-1312.822503	-7.200442	1.751680
-1316.751671	-0.741971	1.756685
-1320.051358	-17.852286	1.761690
-1323.897014	-12.529881	1.766694
-1327.421892	-15.937710	1.771699
-1331.746231	-8.526630	1.776704
-1335.158544	-8.551234	1.781709
-1338.891025	-12.539204	1.786714
-1342.956543	-10.658494	1.791718
-1346.442965	-21.737437	1.796723
-1350.428136	-18.620724	1.801728
-1353.967146	-16.456873	1.806733
-1357.949459	-16.087447	1.811738
-1362.156712	-13.323063	1.816742
-1365.603642	-19.086485	1.821747
-1369.127810	-9.621093	1.826752
-1372.681590	-2.465744	1.831757
-1376.298950	-4.398546	1.836762
-1380.329131	-20.204462	1.841766
-1384.117866	4.876122	1.846771
-1388.368580	-16.157954	1.851776
-1391.424435	10.341157	1.856781
-1395.283550	-21.228929	1.861786
-1399.348305	-6.754076	1.866790
-1402.770366	-13.428103	1.871795
-1406.852088	-26.253379	1.876800
-1410.460429	-16.060152	1.881805
-1414.131421	-18.752222	1.886810
-1417.910416	-21.411226	1.891814
-1421.677709	-5.230524	1.896819
-1425.798244	-26.222276	1.901824
-1429.089860	-13.501610	1.906829
-1433.018461	-22.890208	1.911834
-1437.140751	-21.236768	1.916838
-1440.751978	-8.958459	1.921843
-1444.234308	-12.314576	1.926848
-1448.066691	-26.061145	1.931853
-1451.936877	-6.604616	1.936858
-1455.474865	-12.465275	1.941862
-1458.893991	-17.569157	1.946867
-1463.563516	-17.352842	1.951872
-1466.913366	-14.299816	1.956877
-1470.610184	-34.712811	1.961882
-1474.829072	-8.459466	1.966886
-1478.069440	-26.529842	1.971891
-1481.962148	-21.226457	1.976896
-1485.511994	-12.652429	1.981901
-1489.453374	-21.751895	1.986906
-1493.493105	-29.552059	1.991910
-1497.009993	-17.063295	1.996915
-1501.274099	-15.736046	2.006912
-1501.942714	-14.833211	2.016909
-1499.015565	-15.437722	2.026906
-1496.357343	-12.704104	2.036902
-1494.439556	-16.967790	2.046899
-1492.924599	-12.955366	2.056896
-1490.742661	-10.688595	2.066893
-1488.697286	-19.966611	2.076890
-1486.753512	-11.221568	2.086886
-1485.033775	-13.830474	2.096883
-1483.251947	-20.642747	2.106880
-1480.856975	-9.453261	2.116877
-1479.335033	-18.195902	2.126874
-1477.299350	-10.071845	2.136870
-1475.349343	-22.635955	2.146867
-1473.696167	-13.999095	2.156864
-1471.569921	-13.033833	2.166861
-1469.863433	-24.385858	2.176858
-1467.834401	-13.230916	2.186854
-1465.989544	-26.524975	2.196851
-1464.349204	-14.032080	2.206848
-1462.249819	-6.121878	2.216845
-1460.038937	-17.736235	2.226842
-1458.409174	-13.380613	2.236838
-1456.623302	-12.375046	2.246835
-1454.471108	-13.846933	2.256832
-1452.824134	-24.527879	2.266829
-1450.885316	-17.119297	2.276826
-1448.773646	-12.899248	2.286822
-1447.018371	-16.326925	2.296819
-1445.533908	-12.581148	2.306816
-1443.398662	-3.865138	2.316813
-1441.350062	-19.261685	2.326810
-1439.538961	-13.597797	2.336806
-1437.641020	-20.449155	2.346803
-1435.912237	-13.857929	2.356800
-1434.075470	-11.737930	2.366797
-1432.142063	-12.683743	2.376794
-1430.406691	-18.388083	2.386790
-1428.388821	-20.904163	2.396787
-1426.484879	-20.796897	2.406784
-1424.312185	-10.013836	2.416781
-1422.571513	-15.076427	2.426778
-1420.835217	-0.110576	2.436774
-1418.946528	-15.584133	2.446771
-1417.103408	-9.342755	2.456768
-1415.019803	-13.948698	2.466765
-1413.376854	-9.225700	2.476762
-1411.121840	-12.273915	2.486758
-1409.328780	-10.180054	2.496755
-1408.074952	-9.796594	2.506752
-1405.916654	-19.223669	2.516749
-1403.752974	-8.805435	2.526746
-1402.091777	-13.280586	2.536742
-1400.435108	4.933105	2.546739
-1397.875072	-9.185907	2.556736
-1396.332751	-18.089648	2.566733
-1394.460265	-18.163624	2.576730
-1392.637795	-23.812410	2.586726
-1390.979101	-21.837542	2.596723
-1388.848787	-17.568319	2.606720
-1386.664418	-10.096360	2.616717
-1385.008919	-8.016770	2.626714
-1383.285490	-16.485316	2.636710
-1381.385859	-13.644329	2.646707
-1379.497434	-14.436064	2.656704
-1377.665551	-9.710130	2.666701
-1375.572562	-12.937624	2.676698
-1373.846587	-17.773630	2.686694
-1371.725511	-14.852828	2.696691
-1370.084586	-14.689201	2.706688
-1368.527737	-14.698418	2.716685
-1366.382734	-18.728392	2.726682
-1364.308878	-23.056429	2.736678
-1362.524292	-18.022932	2.746675
-1360.651017	-22.156235	2.756672
-1358.842358	-6.120403	2.766669
-1356.972116	-10.433211	2.776666
-1354.975744	-24.728763	2.786662
-1352.683311	-19.650245	2.796659
-1351.299845	-9.414939	2.806656
-1349.541716	-12.623542	2.816653
-1347.477612	-16.329516	2.826650
-1345.892604	-11.169324	2.836646
-1343.624089	-21.856546	2.846643
-1341.989782	-17.174743	2.856640
-1339.979493	-10.863747	2.866637
-1337.999534	-12.028500	2.876634
-1336.610672	-19.442467	2.886630
-1334.343622	-24.005074	2.896627
-1332.255945	-10.773717	2.906624
-1330.835680	-21.910906	2.916621
-1328.830849	-13.131280	2.926618
-1326.920872	-19.825018	2.936614
-1325.085381	-15.728002	2.946611
-1323.044677	-11.318061	2.956608
-1321.063114	-14.500831	2.966605
-1319.454709	-16.313424	2.976602
-1317.465181	-15.673483	2.986598
-1315.630328	-11.611090	2.996595
-1313.684548	-15.103898	3.006592
-1311.919089	-16.445863	3.016589
-1309.911342	-23.772567	3.026586
-1308.276193	-8.744645	3.036582
-1306.109786	-22.942651	3.046579
-1304.520181	-12.996082	3.056576
-1302.543218	-11.188922	3.066573
-1300.449762	-11.972360	3.076570
-1298.551454	-11.262542	3.086566
-1296.745043	1.060253	3.096563
-1294.926619	-12.073171	3.106560
-1293.287336	-16.380540	3.116557
-1291.239678	-1.034956	3.126554
-1289.405927	-11.733076	3.136550
-1287.482216	-11.560968	3.146547
-1285.498278	-10.179622	3.156544
-1283.795601	-13.066690	3.166541
-1281.829005	-8.423809	3.176538
-1279.916443	-14.284292	3.186534
-1278.123211	-19.274672	3.196531
-1276.179763	-0.096302	3.206528
-1274.511211	-4.591494	3.216525
-1272.431414	-3.416519	3.226522
-1270.340548	-20.174365	3.236518
-1268.609429	-8.677874	3.246515
-1266.753954	-12.865098	3.256512
-1264.854010	-10.199314	3.266509
-1263.393495	-8.175266	3.276506
-1261.062471	-21.273859	3.286502
-1259.111523	-6.967444	3.296499
-1257.570957	-13.016259	3.306496
-1255.668128	-4.777569	3.316493
-1253.761231	-16.036810	3.326490
-1251.707443	-13.844030	3.336486
-1249.803263	-0.216916	3.346483
-1247.854449	-14.031137	3.356480
-1246.130416	-13.212865	3.366477
-1244.330369	-14.405587	3.376474
-1242.281139	-8.719641	3.386470
-1240.568324	-7.817469	3.396467
-1239.188024	-13.981143	3.406464
-1237.066058	0.844218	3.416461
-1234.710759	-4.490276	3.426458
-1232.962105	-1.770254	3.436454
-1231.042405	-5.134095	3.446451
-1229.072230	-4.637814	3.456448
-1227.573803	-2.234567	3.466445
-1225.436736	-2.687041	3.476442
-1223.806956	-14.312421	3.486438
-1221.591247	3.657249	3.496435
-1219.772793	-6.632614	3.506432
-1218.057310	4.083321	3.516429
-1216.117079	-6.920724	3.526426
-1214.197172	0.748465	3.536422
-1212.611538	-8.252104	3.546419
-1210.611969	-3.177090	3.556416
-1208.649710	-3.577894	3.566413
-1206.756968	0.405861	3.576410
-1204.835482	-2.614055	3.586406
-1202.928688	-6.447886	3.596403
-1201.153288	-9.498103	3.606400
-1199.217557	-5.982248	3.616397
-1197.358640	-8.940043	3.626394
-1195.578444	-5.749804	3.636390
-1193.443956	-16.060213	3.646387
-1191.523741	3.846664	3.656384
-1189.878794	-3.312964	3.666381
-1188.381658	-5.535536	3.676378
-1186.118348	-6.388678	3.686374
-1184.103683	-10.149758	3.696371
-1182.194654	-16.885866	3.706368
-1180.761507	-4.773231	3.716365
-1178.646716	-7.975624	3.726362
-1176.605589	-9.048982	3.736358
-1174.915867	-8.289899	3.746355
-1173.170756	-6.221333	3.756352
-1171.059518	-12.364560	3.766349
-1169.210705	-4.241878	3.776346
-1167.227589	-20.641378	3.786342
-1165.423951	6.111154	3.796339
-1163.638087	-9.544731	3.806336
-1161.644350	-21.210934	3.816333
-1160.056322	-4.825417	3.826330
-1157.934213	-1.539859	3.836326
-1155.939364	-5.013553	3.846323
-1154.160368	-10.058408	3.856320
-1152.464759	-1.930145	3.866317
-1150.345901	2.827437	3.876314
-1148.615476	-11.283339	3.886310
-1146.549567	-1.678086	3.896307
-1144.813847	-6.687592	3.906304
-1142.855821	-8.832301	3.916301
-1140.889345	-9.124781	3.926298
-1139.413806	-10.598646	3.936294
-1137.522941	-5.815632	3.946291
-1135.526467	-17.341738	3.956288
-1133.457904	-8.992093	3.966285
-1131.642976	-11.985428	3.976282
-1129.957480	-12.416095	3.986278
-1128.041075	1.371805	3.996275
-1125.924750	-12.533865	4.006272
-1124.072002	-4.478084	4.016269
-1122.306435	-11.619070	4.026266
-1120.302928	-10.295970	4.036262
-1118.531045	-7.443795	4.046259
-1116.866078	-17.900069	4.056256
-1114.571648	-11.566426	4.066253
-1112.831013	-5.081032	4.076250
-1111.128249	-15.458093	4.086246
-1109.359715	-12.202767	4.096243
-1107.249319	-20.298849	4.106240
-1105.383425	-13.470353	4.116237
-1103.540982	-8.820082	4.126234
-1101.705522	-14.251278	4.136230
-1099.913601	-10.909690	4.146227
-1097.884038	-13.201587	4.156224
-1096.219678	-7.706553	4.166221
-1094.060682	-7.502452	4.176218
-1091.945894	-13.333566	4.186214
-1090.284725	-12.626694	4.196211
-1088.789725	-11.009079	4.206208
-1086.868668	-6.955546	4.216205
-1085.070379	-9.284644	4.226202
-1082.604309	-5.124088	4.236198
-1080.749230	-13.015111	4.246195
-1079.146395	-13.831971	4.256192
-1077.359722	-4.481968	4.266189
-1075.304696	-7.035273	4.276186
-1073.522047	-10.992821	4.286182
-1071.694257	-5.350235	4.296179
-1069.951432	-17.105706	4.306176
-1067.727260	-15.074215	4.316173
-1066.163972	-12.968590	4.326170
-1063.999444	-6.955146	4.336166
-1062.317207	-14.456950	4.346163
-1060.519254	-18.175370	4.356160
-1058.429465	-20.595280	4.366157
-1056.504427	-16.989177	4.376154
-1054.694595	-25.179237	4.386150
-1052.798817	-19.792237	4.396147
-1051.159719	-9.217100	4.406144
-1049.209406	-15.714990	4.416141
-1047.409127	-19.015374	4.426138
-1045.168703	-12.974582	4.436134
-1043.313419	-16.678476	4.446131
-1041.677931	-21.157168	4.456128
-1039.775318	-18.515304	4.466125
-1037.772093	-19.621951	4.476122
-1036.159662	-8.551511	4.486118
-1034.207885	-14.473340	4.496115
-1032.197016	-22.153991	4.506112
-1030.445215	-18.648047	4.516109
-1028.489475	-17.037770	4.526106
-1026.612052	-14.916047	4.536102
-1024.674812	-21.740227	4.546099
-1022.785840	-26.062088	4.556096
-1021.023734	-11.161585	4.566093
-1019.151708	-22.628227	4.576090
-1017.276583	-19.247779	4.586086
-1015.409641	-22.926675	4.596083
-1013.528101	-20.650872	4.606080
-1011.650604	-21.955271	4.616077
-1009.741519	-17.456101	4.626074
-1007.768896	-20.214051	4.636070
-1005.959738	-16.560952	4.646067
-1004.084244	-21.971636	4.656064
-1002.171807	-23.592651	4.666061
-1000.086072	-15.949796	4.676058
-998.387242	-20.474903	4.686054
-996.588017	-23.506675	4.696051
-994.936972	-20.156685	4.706048
-992.868057	-19.754937	4.716045
-990.974978	-28.352979	4.726042
-988.959983	-15.632245	4.736038
-987.104977	-23.744225	4.746035
-985.476135	-13.380543	4.756032
-983.586799	-17.355086	4.766029
-981.767010	-17.088742	4.776026
-979.644140	-32.280521	4.786022
-977.561087	-26.097664	4.796019
-975.914137	-21.038681	4.806016
-974.151418	-29.219571	4.816013
-972.037641	-17.027746	4.826010
-970.194967	-18.264969	4.836006
-968.550116	-26.944873	4.846003
-966.664884	-15.782225	4.856000
-964.822766	-22.152225	4.865997
-962.634047	-18.420848	4.875994
-960.947028	-20.128935	4.885990
-959.447245	-18.527789	4.895987
-957.010127	-27.688039	4.905984
-955.277338	-19.379265	4.915981
-953.611123	-22.336055	4.925978
-951.645524	-22.861908	4.935974
-949.315159	-24.897057	4.945971
-947.538543	-15.767960	4.955968
-946.026483	-17.891720	4.965965
-944.317959	-14.044068	4.975962
-942.150842	-17.276724	4.985958
-940.344367	-16.652975	4.995955
-938.166031	-22.146770	5.005952
-936.675289	-11.310990	5.015949
-934.468737	-15.558837	5.025946
-932.956791	-12.393388	5.035942
-931.056185	-13.950880	5.045939
-928.896811	-16.080242	5.055936
-927.040891	-16.910624	5.065933
-925.331528	-13.940938	5.075930
-923.560424	-13.016273	5.085926
-921.643919	-18.933954	5.095923
-919.836323	-14.680568	5.105920
-917.842953	-6.476574	5.115917
-915.681001	-12.166669	5.125914
-913.759575	-22.918021	5.135910
-912.034652	-15.196865	5.145907
-910.327876	-9.215865	5.155904
-908.532322	-18.181925	5.165901
-906.592058	-8.521615	5.175898
-904.721624	-8.888537	5.185894
-902.604869	-23.818779	5.195891
-900.893277	-27.378017	5.205888
-899.198058	-28.051639	5.215885
-897.218961	-13.580432	5.225882
-895.034565	-21.021894	5.235878
-893.484570	-27.210934	5.245875
-891.505380	-16.402693	5.255872
-889.660406	-25.427160	5.265869
-887.881091	-17.878883	5.275866
-885.782286	-23.483068	5.285862
-883.732382	-17.157456	5.295859
-882.360876	-18.646107	5.305856
-880.443052	-8.529053	5.315853
-878.408209	-14.629823	5.325850
-876.560407	-21.548535	5.335846
-874.466858	-22.562121	5.345843
-872.592322	-16.216357	5.355840
-870.880319	-14.898540	5.365837
-869.091617	-12.628299	5.375834
-867.282794	-16.405156	5.385830
-864.977571	-21.890752	5.395827
-863.315066	-24.728473	5.405824
-861.621132	-21.464184	5.415821
-859.782320	-24.148519	5.425818
-857.535107	-23.285708	5.435814
-855.758852	-20.171936	5.445811
-854.159534	-22.263800	5.455808
-852.229409	-19.146203	5.465805
-850.307330	-22.098039	5.475802
-848.244806	-23.030858	5.485798
-846.167690	-22.835543	5.495795
-844.385424	-18.822771	5.505792
-843.227559	-19.348877	5.515789
-840.843241	-9.768965	5.525786
-838.837048	-19.084422	5.535782
-836.823993	-7.018445	5.545779
-835.152615	-17.854505	5.555776
-833.344624	-22.070126	5.565773
-831.646038	-9.376014	5.575770
-829.793990	-27.789484	5.585766
-827.758728	-22.299857	5.595763
-825.739920	-17.459665	5.605760
-823.805097	-13.475998	5.615757
-822.204588	-24.079677	5.625754
-820.189663	-19.324118	5.635750
-818.319247	-22.592916	5.645747
-816.184288	-12.862600	5.655744
-814.690307	-13.268744	5.665741
-812.850437	-25.060089	5.675738
-810.675751	-11.906829	5.685734
-808.865905	-18.401028	5.695731
-807.069567	-12.934763	5.705728
-805.306105	-17.430601	5.715725
-803.560634	-20.264176	5.725722
-801.375842	-16.075722	5.735718
-799.518948	-22.848998	5.745715
-797.492161	-20.864639	5.755712
-795.777435	-13.575944	5.765709
-794.028604	-10.314060	5.775706
-792.267438	-20.821831	5.785702
-790.263369	-18.423330	5.795699
-788.299451	-19.847151	5.805696
-786.298750	-25.680295	5.815693
-784.673405	-15.811656	5.825690
-782.541489	-15.254010	5.835686
-780.665258	-25.265452	5.845683
-778.970986	-15.939901	5.855680
-777.314867	-17.145579	5.865677
-775.371836	-20.804878	5.875674
-773.094567	-24.121301	5.885670
-771.359442	-16.709540	5.895667
-769.575380	-16.251014	5.905664
-767.655696	-17.323557	5.915661
-765.891352	-14.994082	5.925658
-763.791744	-16.287999	5.935654
-761.946517	-19.199064	5.945651
-760.194323	-17.878116	5.955648
-757.986323	-23.288078	5.965645
-756.500167	-27.887972	5.975642
-754.498267	-7.906873	5.985638
-752.504871	-27.504933	5.995635
-750.905420	-20.483557	6.005632
-749.319702	-20.710121	6.015629
-747.094750	-13.657658	6.025626
-745.037121	-22.929161	6.035622
-743.015135	-20.891885	6.045619
-741.553748	-17.007739	6.055616
-739.378611	-11.213554	6.065613
-737.648217	-4.476756	6.075610
-735.850796	-11.322589	6.085606
-733.812971	-18.402615	6.095603
-732.029383	-7.870832	6.105600
-730.139531	-14.177249	6.115597
-728.292772	-7.670609	6.125594
-726.438205	-17.839601	6.135590
-724.423012	-20.937265	6.145587
-722.578713	-25.234393	6.155584
-720.703401	-8.074981	6.165581
-718.944711	-15.727725	6.175578
-716.856654	-15.439313	6.185574
-715.193449	-9.043848	6.195571
-713.520990	-10.528395	6.205568
-711.439871	-15.472804	6.215565
-709.619848	-10.799675	6.225562
-707.578847	-9.834295	6.235558
-705.792517	-17.553023	6.245555
-703.694145	-13.015944	6.255552
-701.562326	-9.014705	6.265549
-699.974355	-9.273173	6.275546
-698.394394	-16.913132	6.285542
-696.705209	-28.741896	6.295539
-694.638224	-15.517623	6.305536
-692.745255	-22.036075	6.315533
-690.626883	-20.593597	6.325530
-688.851901	-24.195977	6.335526
-686.924485	-18.017967	6.345523
-685.265437	-16.944170	6.355520
-683.289645	-13.112183	6.365517
-681.152588	-6.748200	6.375514
-679.277776	-34.327368	6.385510
-677.723705	-17.012388	6.395507
-675.692258	-17.899042	6.405504
-673.913250	-22.397271	6.415501
-672.249810	-19.165858	6.425498
-670.149892	-32.012289	6.435494
-668.088902	-13.932025	6.445491
-666.304121	-22.125714	6.455488
-664.448411	-22.876916	6.465485
-662.532162	-16.322909	6.475482
-660.712956	-22.786922	6.485478
-658.841189	-15.966871	6.495475
-657.054370	-13.607747	6.505472
-654.947578	-24.268542	6.515469
-653.310677	1.219659	6.525466
-651.186155	-19.098739	6.535462
-649.506576	-15.424648	6.545459
-647.437837	-15.905152	6.555456
-645.922070	-18.180890	6.565453
-643.813916	-18.402439	6.575450
-642.147790	-12.528412	6.585446
-639.892046	-23.596659	6.595443
-638.246002	-15.330599	6.605440
-636.164167	-13.373838	6.615437
-634.358540	-21.913451	6.625434
-632.731533	-21.366575	6.635430
-630.807019	-19.272576	6.645427
-628.823458	-17.363263	6.655424
-626.811926	-24.783195	6.665421
-625.119377	-20.710127	6.675418
-623.206412	-32.726169	6.685414
-621.365176	-21.592490	6.695411
-619.608015	-24.841465	6.705408
-617.628569	-18.876959	6.715405
-615.542503	-22.816340	6.725402
-614.260486	-10.216533	6.735398
-611.662167	-23.662000	6.745395
-610.029131	-30.585680	6.755392
-608.273948	-24.487451	6.765389
-606.441141	-16.145420	6.775386
-604.154768	-21.310415	6.785382
-602.597342	-16.230530	6.795379
-600.523741	-16.804923	6.805376
-598.956126	-30.763044	6.815373
-596.708364	-18.794332	6.825370
-594.935655	-24.297236	6.835366
-593.580449	-22.006474	6.845363
-591.242924	-22.397244	6.855360
-589.302746	-18.627378	6.865357
-587.685383	-14.818571	6.875354
-585.708063	-18.328472	6.885350
-583.425372	-25.908523	6.895347
-581.883490	-22.570789	6.905344
-580.252760	-16.861579	6.915341
-578.126666	-21.820955	6.925338
-576.364505	-12.172940	6.935334
-574.265659	-24.667047	6.945331
-572.438531	-19.203932	6.955328
-570.637960	-17.491115	6.965325
-568.984404	-14.349621	6.975322
-567.090043	-26.253717	6.985318
-565.164378	-20.724235	6.995315
-563.108552	-20.348437	7.005312
-561.196766	-20.606436	7.015309
-559.385741	-18.590560	7.025306
-557.725464	-13.179720	7.035302
-555.436893	-16.677740	7.045299
-553.528351	-21.630764	7.055296
-551.869644	-22.287255	7.065293
-550.026070	-14.344768	7.075290
-548.163267	-13.478674	7.085286
-546.262583	-14.923775	7.095283
-544.364120	-19.076277	7.105280
-542.333034	-17.401837	7.115277
-541.024548	-18.090796	7.125274
-538.843839	-11.839434	7.135270
-536.995090	-18.789637	7.145267
-534.967669	-19.948672	7.155264
-533.302514	-25.113844	7.165261
-531.044219	-10.211624	7.175258
-529.374710	-18.225769	7.185254
-527.544034	-13.489459	7.195251
-525.581549	-17.574809	7.205248
-523.523274	-19.938701	7.215245
-521.929930	-23.736150	7.225242
-520.259832	-20.227809	7.235238
-518.034972	-16.711762	7.245235
-515.958351	-16.100835	7.255232
-514.344129	-24.470856	7.265229
-512.898215	-10.266188	7.275226
-510.683193	-13.671897	7.285222
-508.577560	-28.696383	7.295219
-506.865185	-22.905429	7.305216
-504.899895	-17.298542	7.315213
-503.215970	-11.152527	7.325210
-501.197482	-8.973959	7.335206
-499.241882	-13.025033	7.345203
-497.491664	-14.210813	7.355200
-495.732800	-21.118211	7.365197
-493.873439	-8.938934	7.375194
-491.800741	-20.143609	7.385190
-489.334329	-13.513112	7.395187
-488.112185	-15.945533	7.405184
-486.575817	-23.303681	7.415181
-484.437413	-22.519445	7.425178
-482.463189	-11.566338	7.435174
-480.668945	-16.693677	7.445171
-478.910487	-21.411109	7.455168
-476.724838	-11.240145	7.465165
-474.792068	-22.967167	7.475162
-473.316408	-12.760178	7.485158
-471.356238	-8.401325	7.495155
-468.974085	-15.484033	7.505152
-467.415139	-13.865174	7.515149
-465.694243	-11.577474	7.525146
-463.813339	-10.564210	7.535142
-461.994584	-14.489196	7.545139
-459.631067	-21.223145	7.555136
-458.175187	-13.828107	7.565133
-456.025039	-11.754206	7.575130
-454.210092	-17.086928	7.585126
-452.668239	-7.657821	7.595123
-450.429154	-15.336582	7.605120
-448.680938	-14.922613	7.615117
-447.347026	-6.161312	7.625114
-444.760182	-20.332651	7.635110
-442.518697	-16.746558	7.645107
-441.083268	-16.020542	7.655104
-439.522905	-18.480109	7.665101
-437.487559	-15.832096	7.675098
-435.575039	-11.896636	7.685094
-433.899801	-3.442448	7.695091
-431.774249	-12.454579	7.705088
-429.800284	-14.561785	7.715085
-428.033654	-20.807253	7.725082
-426.232277	-13.547886	7.735078
-424.357793	-15.394478	7.745075
-422.426800	-14.663903	7.755072
-420.517343	-6.971809	7.765069
-418.448368	-13.185030	7.775066
-416.815648	-17.108696	7.785062
-414.883408	-18.094546	7.795059
-412.866158	-21.718048	7.805056
-411.304239	-16.218766	7.815053
-409.246281	-14.087471	7.825050
-407.632752	-23.043080	7.835046
-405.695318	-18.217935	7.845043
-403.791539	-18.686099	7.855040
-401.558111	-23.847193	7.865037
-400.084271	-14.494028	7.875034
-397.759777	-21.602197	7.885030
-395.930725	-13.988821	7.895027
-394.355146	-11.726810	7.905024
-392.482247	-14.139939	7.915021
-390.595202	-13.449687	7.925018
-388.534637	-6.190618	7.935014
-386.771183	-16.559564	7.945011
-384.824383	-19.322364	7.955008
-383.057456	-11.607481	7.965005
-381.347165	-17.250269	7.975002
-379.540559	-5.891369	7.984998
-377.277901	-16.729994	7.994995
-375.285192	-20.242185	8.004992
-373.732074	-12.960504	8.014989
-371.630387	-10.026197	8.024986
-369.940470	-15.190485	8.034982
-367.793373	-19.718850	8.044979
-366.140698	-13.701945	8.054976
-364.285872	-12.605496	8.064973
-362.538575	-18.816257	8.074970
-360.631959	-18.935909	8.084966
-358.591020	-21.633196	8.094963
-356.606511	-14.732993	8.104960
-354.821847	-14.924745	8.114957
-353.261092	-15.161270	8.124954
-351.561032	-9.601896	8.134950
-349.324073	-27.310791	8.144947
-347.144367	-18.243959	8.154944
-345.258464	-9.911754	8.164941
-343.798387	-6.897092	8.174938
-341.649814	-19.125827	8.184934
-339.736896	-16.072939	8.194931
-337.852212	-15.529103	8.204928
-336.147560	-15.392294	8.214925
-334.335113	-16.815249	8.224922
-332.301139	-16.903108	8.234918
-330.466619	-17.380682	8.244915
-328.768025	-14.040950	8.254912
-327.044498	-9.236845	8.264909
-324.860958	-7.854962	8.274906
-322.927289	-18.707334	8.284902
-321.156760	-5.350087	8.294899
-319.137959	-12.766214	8.304896
-317.020323	-9.357584	8.314893
-315.473891	-20.283915	8.324890
-313.689700	-7.863537	8.334886
-311.671295	-19.403605	8.344883
-309.660729	-15.343172	8.354880
-308.090906	-19.910380	8.364877
-306.048236	-11.710531	8.374874
-304.176505	-12.850836	8.384870
-302.420545	-10.115475	8.394867
-300.401176	-11.819319	8.404864
-298.818439	-14.947075	8.414861
-296.723327	-8.768647	8.424858
-294.797378	-10.962814	8.434854
-292.638424	-16.846102	8.444851
-291.206244	-17.231003	8.454848
-289.148462	-10.685049	8.464845
-287.668639	-19.461361	8.474842
-285.551017	-5.439522	8.484838
-283.337188	-18.239129	8.494835
-281.698828	-6.041747	8.504832
-279.807886	-21.044439	8.514829
-277.992299	-10.086340	8.524826
-276.046579	-18.521770	8.534822
-274.278331	-21.563863	8.544819
-272.347655	-15.701784	8.554816
-270.261269	-12.809151	8.564813
-268.560438	-14.105299	8.574810
-266.732934	-17.284735	8.584807
-264.930838	-22.381599	8.594803
-262.778099	-14.414005	8.604800
-260.918137	-17.609669	8.614797
-259.324736	-10.414856	8.624794
-257.416846	-10.144648	8.634791
-255.337428	-14.717378	8.644787
-253.280052	-18.945551	8.654784
-251.719341	-16.021101	8.664781
-249.809758	-9.563556	8.674778
-247.939522	-14.556029	8.684775
-246.243787	-7.683839	8.694771
-244.401937	-17.406818	8.704768
-242.301631	-17.753071	8.714765
-240.389107	-9.409234	8.724762
-238.435070	-21.003710	8.734759
-236.765558	-13.446837	8.744755
-234.687377	-13.189580	8.754752
-232.923064	-25.350582	8.764749
-230.844527	-8.371540	8.774746
-229.188641	-14.354478	8.784743
-227.383456	-14.754664	8.794739
-225.338660	-18.865549	8.804736
-223.587881	-21.364844	8.814733
-221.612435	-20.866980	8.824730
-219.683626	-20.787967	8.834727
-217.716177	-26.478002	8.844723
-215.859834	-17.075232	8.854720
-214.256456	-18.019490	8.864717
-211.985061	-18.077247	8.874714
-210.547635	-17.694026	8.884711
-208.898082	-17.366762	8.894707
-206.550910	-21.715352	8.904704
-204.638209	-6.700772	8.914701
-202.773980	-21.225492	8.924698
-201.149620	-13.239825	8.934695
-199.022523	-18.767442	8.944691
-197.516706	-10.173933	8.954688
-195.415082	-19.946230	8.964685
-193.344245	-24.724370	8.974682
-191.778287	-26.196299	8.984679
-189.815409	-26.770037	8.994675
-188.038885	-22.162173	9.004672
-185.950965	-34.245315	9.014669
-184.128256	-21.027335	9.024666
-182.162319	-18.699586	9.034663
-180.228599	-30.076046	9.044659
-178.685708	-20.891633	9.054656
-176.417595	-28.524265	9.064653
-174.878331	-11.321748	9.074650
-173.038723	-14.883556	9.084647
-171.047277	-23.960913	9.094643
-168.896553	-24.054634	9.104640
-167.311421	-22.232921	9.114637
-165.462726	-19.769613	9.124634
-163.867857	-17.914716	9.134631
-161.645535	-19.571888	9.144627
-159.581269	-8.665998	9.154624
-157.922924	-18.220697	9.164621
-156.039199	-19.552267	9.174618
-154.056768	-13.349411	9.184615
-152.220867	-20.660438	9.194611
-150.382853	-20.093219	9.204608
-148.498017	-20.488689	9.214605
-146.520258	-18.072800	9.224602
-144.796417	-17.405258	9.234599
-142.735760	-9.212860	9.244595
-140.838602	-13.383801	9.254592
-139.183819	-18.404971	9.264589
-137.410562	-15.154375	9.274586
-135.714457	-26.270272	9.284583
-133.349341	-21.435771	9.294579
-131.245463	-3.597017	9.304576
-129.664653	-15.389228	9.314573
-128.358395	-13.682457	9.324570
-125.825249	-19.019025	9.334567
-123.992260	-33.587644	9.344563
-122.243658	-19.663078	9.354560
-120.363993	-14.057978	9.364557
-118.372872	-7.918051	9.374554
-116.519747	-8.652631	9.384551
-114.746740	-16.825138	9.394547
-112.839799	-20.471852	9.404544
-110.976392	-5.981397	9.414541
-109.013115	-8.983444	9.424538
-107.332138	-19.939029	9.434535
-105.688102	-12.940068	9.444531
-103.300988	-17.282306	9.454528
-101.649683	-15.081124	9.464525
-99.679948	-11.699222	9.474522
-97.664124	-9.363571	9.484519
-96.125222	-15.960891	9.494515
-94.074412	-17.450118	9.504512
-92.191716	-9.679259	9.514509
-90.291071	-16.787427	9.524506
-88.484241	-9.375497	9.534503
-86.474213	-2.905412	9.544499
-84.689158	-12.751855	9.554496
-82.993227	-15.198094	9.564493
-81.156326	-9.000373	9.574490
-79.200664	-8.376083	9.584487
-77.000962	-20.210160	9.594483
-75.634183	-1.361684	9.604480
-73.204529	-20.212659	9.614477
-71.367179	-16.940660	9.624474
-69.698993	-13.917975	9.634471
-67.814083	-21.241500	9.644467
-65.965010	-18.426083	9.654464
-64.058235	-14.595180	9.664461
-62.126234	-23.160893	9.674458
-60.569331	-17.104797	9.684455
-58.279439	-16.544863	9.694451
-56.643179	-15.236471	9.704448
-54.698492	-24.437331	9.714445
-52.807991	-19.029685	9.724442
-51.150251	-17.009486	9.734439
-49.019894	-15.153097	9.744435
-46.813385	-19.338581	9.754432
-45.327185	-18.852521	9.764429
-43.505429	-18.369465	9.774426
-41.728941	-11.888930	9.784423
-39.745718	-10.370623	9.794419
-37.589403	-18.089513	9.804416
-35.724594	-8.991075	9.814413
-34.201133	-19.329412	9.824410
-32.249787	-7.409113	9.834407
-30.047373	-17.239994	9.844403
-28.713040	-14.795574	9.854400
-26.676808	-22.059528	9.864397
-24.705030	-16.363257	9.874394
-22.917566	-11.384390	9.884391
-20.688371	-9.968459	9.894387
-18.947906	-13.530130	9.904384
-16.815566	-13.879720	9.914381
-15.430978	-8.763953	9.924378
-13.628363	-3.211202	9.934375
-11.589296	-7.044702	9.944371
-9.453798	-13.224003	9.954368
-7.629368	-14.803359	9.964365
-6.166320	-9.269069	9.974362
-4.541624	17.925346	9.984359
-3.237462	39.456965	9.994355
-1.850868	90.889057	10.004352
-0.599072	143.896466	10.014349
0.000000	221.794012	10.019354
0.787821	246.480645	10.024359
1.342978	288.767834	10.029363
2.048480	336.364226	10.034368
2.478044	364.066463	10.039373
2.930909	390.817319	10.044378
3.650616	407.091285	10.049383
3.540767	420.274393	10.054387
3.725733	437.029490	10.059392
4.075661	454.125714	10.064397
4.075010	471.164340	10.069402
4.259669	472.437425	10.074407
4.350841	476.719977	10.079411
4.431190	474.089499	10.084416
4.777989	483.661239	10.089421
4.322480	488.103530	10.094426
4.494817	505.592408	10.099431
4.327843	485.093948	10.104435
4.403502	503.066587	10.109440
4.416345	511.929964	10.114445
4.632587	523.012739	10.119450
4.949091	518.368710	10.124455
5.159890	540.154899	10.129459
5.268488	521.716041	10.134464
4.948646	556.161229	10.139469
5.103018	521.124305	10.144474
5.138167	555.080793	10.149479
5.129230	529.465188	10.154483
5.257433	545.120892	10.159488
5.314059	551.443201	10.164493
5.314542	554.496052	10.169498
5.494574	546.833480	10.174503
5.080901	562.723864	10.179507
5.389264	534.837335	10.184512
5.172481	565.267045	10.189517
5.606670	550.398405	10.194522
5.501194	550.818931	10.199527
5.054065	584.275260	10.204531
5.380551	557.147452	10.209536
5.343281	585.503305	10.214541
5.195501	556.776452	10.219546
5.527305	585.390397	10.224551
5.664657	576.141926	10.229555
5.784728	586.942052	10.234560
5.680582	600.069221	10.239565
5.883148	597.524881	10.244570
6.124847	587.217411	10.249575
6.092060	598.964428	10.254579
5.881041	601.029177	10.259584
5.955597	597.363561	10.264589
6.081715	605.136619	10.269594
6.266109	606.815029	10.274599
6.222815	603.810018	10.279603
6.458910	598.313057	10.284608
5.965318	610.146198	10.289613
6.390610	600.173705	10.294618
6.437968	597.229929	10.299623
6.254017	614.717422	10.304627
6.424441	613.025016	10.309632
6.372554	610.770414	10.314637
6.247445	606.584719	10.319642
6.402614	618.189810	10.324647
6.590057	634.880088	10.329651
7.120279	634.011793	10.334656
7.060851	635.820558	10.339661
6.601533	636.207641	10.344666
6.806993	647.683311	10.349671
6.970197	652.023810	10.354675
6.868438	654.172062	10.359680
6.977141	665.022945	10.364685
6.859176	647.556761	10.369690
6.839346	658.076485	10.374695
6.871198	662.676055	10.379699
7.001974	662.166358	10.384704
7.260636	637.203307	10.389709
6.537791	677.390008	10.394714
7.153445	653.819188	10.399719
6.902919	664.210135	10.404723
7.104808	678.644724	10.409728
7.312065	689.852062	10.414733
7.516046	701.116700	10.419738
7.223756	688.902662	10.424743
7.302133	700.305605	10.429747
7.567145	709.890541	10.434752
7.508237	701.095913	10.439757
7.391119	703.204044	10.444762
7.343634	712.682710	10.449767
7.561744	704.993481	10.454771
7.486277	713.927837	10.459776
7.779364	736.186894	10.464781
7.915441	738.688303	10.469786
7.998722	734.073521	10.474791
8.151949	752.306907	10.479795
8.242048	743.496371	10.484800
8.527509	722.100670	10.489805
8.010681	738.453972	10.494810
8.448315	707.338998	10.499815
8.029978	710.651070	10.504819
8.078499	708.400938	10.509824
8.193920	712.753808	10.514829
8.499662	750.193625	10.519834
8.916518	738.293785	10.524839
8.276674	720.188517	10.529843
8.077584	731.164236	10.534848
8.667275	715.043767	10.539853
8.390860	769.563269	10.544858
8.614283	735.423132	10.549863
8.873599	780.635285	10.554867
9.041015	743.017440	10.559872
8.723028	762.369934	10.564877
9.039969	749.718050	10.569882
9.218745	720.653359	10.574887
8.555385	751.671924	10.579891
8.615262	723.625973	10.584896
8.826010	725.867891	10.589901
8.388384	755.951606	10.594906
8.931104	758.243080	10.599911
8.671485	744.371148	10.604915
8.751104	771.070279	10.609920
8.765495	762.866314	10.614925
9.003312	763.356668	10.619930
9.361874	769.846955	10.624935
9.348533	786.484278	10.629939
9.451917	786.992921	10.634944
9.551722	772.065428	10.639949
9.171355	782.869828	10.644954
9.715691	777.810911	10.649959
9.319035	788.756685	10.654963
9.287888	795.564607	10.659968
9.532873	788.875562	10.664973
9.406553	800.016345	10.669978
9.498294	794.852993	10.674983
9.373509	795.079488	10.679987
9.358542	800.683199	10.684992
9.516184	791.371430	10.689997
9.603334	810.342401	10.695002
9.896593	813.944694	10.700007
10.144248	828.977680	10.705011
10.501190	819.523718	10.710016
10.364093	813.863852	10.715021
9.930934	799.136456	10.720026
9.893868	811.231256	10.725031
10.030567	820.155490	10.730035
10.159505	821.208838	10.735040
10.430071	832.204339	10.740045
10.445221	832.665557	10.745050
10.568724	832.138091	10.750055
10.194974	853.770408	10.755059
10.882476	828.109424	10.760064
10.655153	811.922045	10.765069
10.121426	830.555259	10.770074
10.674982	817.666880	10.775079
10.549030	831.928409	10.780083
10.523229	847.812431	10.785088
10.713451	839.443183	10.790093
10.393035	841.612146	10.795098
10.601669	832.339526	10.800103
10.606235	837.795057	10.805107
10.593353	847.601028	10.810112
10.917790	849.364362	10.815117
10.906733	840.454784	10.820122
11.285567	837.096966	10.825127
11.154144	835.108905	10.830131
10.701448	845.070181	10.835136
10.856192	848.740307	10.840141
10.913616	840.362278	10.845146
11.186732	874.488139	10.850151
11.165955	880.307274	10.855155
11.425220	859.350789	10.860160
11.367163	882.391477	10.865165
11.313711	882.504093	10.870170
11.916544	866.124318	10.875175
11.832699	875.479579	10.880179
11.718241	860.054736	10.885184
11.623485	844.224645	10.890189
11.436778	847.474571	10.895194
11.450029	849.585584	10.900199
11.544724	876.758745	10.905203
11.634523	872.087686	10.910208
11.732993	883.724111	10.915213
11.887833	884.796986	10.920218
12.102072	879.303406	10.925223
11.789054	878.847141	10.930227
12.189304	877.400322	10.935232
12.104165	888.714376	10.940237
12.243472	887.556759	10.945242
12.277098	872.294365	10.950247
12.048831	872.256668	10.955251
12.004308	888.287223	10.960256
12.464534	880.627093	10.965261
11.947360	877.850574	10.970266
12.573595	877.550427	10.975271
12.494643	888.079747	10.980275
12.092511	890.130864	10.985280
12.619876	886.265218	10.990285
12.540801	885.937219	10.995290
12.565222	874.806339	11.000295
12.105933	877.573046	11.005299
12.376311	886.405036	11.010304
12.448900	879.590483	11.015309
11.961332	878.580162	11.020314
12.320542	913.548671	11.025319
12.797852	911.906630	11.030323
13.019070	906.885014	11.035328
13.046778	932.490429	11.040333
13.430872	894.178462	11.045338
13.236077	907.224173	11.050343
13.164069	907.232516	11.055347
12.979332	892.769753	11.060352
13.080510	915.029733	11.065357
12.966661	906.041893	11.070362
12.817815	905.909526	11.075367
12.769702	917.563051	11.080371
12.839056	904.608323	11.085376
13.070882	920.322022	11.090381
12.923350	913.290249	11.095386
13.303102	929.409296	11.100391
13.515960	940.735785	11.105395
13.694523	931.633479	11.110400
13.851742	937.693907	11.115405
13.550162	957.936604	11.120410
14.051054	924.251664	11.125415
13.758299	920.080002	11.130419
13.610189	917.604155	11.135424
13.689161	917.069597	11.140429
13.626997	931.608056	11.145434
13.973669	929.141600	11.150439
14.217024	938.433675	11.155443
14.085473	934.179526	11.160448
13.915538	937.776882	11.165453
13.764949	941.511503	11.170458
14.502970	938.719272	11.175463
14.083678	929.953600	11.180467
14.082823	948.530357	11.185472
14.392782	921.937517	11.190477
14.052674	964.971879	11.195482
14.820304	918.548272	11.200487
14.270406	961.657087	11.205491
14.326023	924.118106	11.210496
14.804868	971.695975	11.215501
14.236529	942.133412	11.220506
14.692888	952.615244	11.225511
14.635741	941.147237	11.230515
14.729396	937.998887	11.235520
14.758835	931.534969	11.240525
14.633370	943.825330	11.245530
14.877076	934.182773	11.250535
14.640668	957.515380	11.255539
14.710653	947.285507	11.260544
14.854124	938.595650	11.265549
14.404523	948.756777	11.270554
14.705822	945.102217	11.275559
14.794097	955.011976	11.280563
14.797049	956.779292	11.285568
14.753514	949.226285	11.290573
15.150439	946.695040	11.295578
15.001676	940.297389	11.300583
15.147233	952.987655	11.305587
15.018642	982.284528	11.310592
15.646643	970.741909	11.315597
15.328610	976.643188	11.320602
15.539257	968.011986	11.325607
15.637985	979.263668	11.330611
15.666377	971.932568	11.335616
15.762509	946.627476	11.340621
15.308089	939.545290	11.345626
15.452887	953.385283	11.350631
15.479600	959.640001	11.355635
15.758140	957.343681	11.360640
15.609795	985.894654	11.365645
15.596666	978.898182	11.370650
15.946478	977.815793	11.375655
15.858627	977.285763	11.380659
16.277207	968.943097	11.385664
16.192084	965.506286	11.390669
16.021853	969.548401	11.395674
16.260698	962.366666	11.400679
16.178588	987.492951	11.405683
15.940363	958.361830	11.410688
16.038042	966.294161	11.415693
15.687484	983.438085	11.420698
15.859734	981.452030	11.425703
15.839159	977.148628	11.430707
15.790313	969.052405	11.435712
16.406454	991.436948	11.440717
16.540408	984.899566	11.445722
16.490749	1011.164017	11.450727
16.598814	1009.497281	11.455731
16.370440	1012.063177	11.460736
16.732675	1000.750583	11.465741
16.438755	1000.788013	11.470746
16.823412	1024.215635	11.475751
16.642302	1007.930777	11.480755
16.552931	1002.340495	11.485760
16.631379	1019.780316	11.490765
16.678905	1000.636222	11.495770
16.883459	1013.511099	11.500775
16.643753	1016.067764	11.505779
16.788432	1010.459072	11.510784
17.022804	1010.057420	11.515789
17.275352	1025.061446	11.520794
17.705350	1012.922742	11.525799
17.365205	1002.012339	11.530803
17.434464	1008.835886	11.535808
17.469293	1006.475927	11.540813
17.085584	1005.130483	11.545818
17.392243	994.591589	11.550823
17.204023	1002.574271	11.555827
17.270342	1002.809711	11.560832
17.435200	1010.799162	11.565837
17.264736	1029.915590	11.570842
17.653904	1031.788473	11.575847
17.567189	1031.988398	11.580851
17.712511	1035.223254	11.585856
18.285245	1028.909184	11.590861
18.021280	1025.273800	11.595866
18.115785	1003.662134	11.600871
18.004590	1002.916628	11.605875
17.615958	1000.439706	11.610880
17.998292	1004.078303	11.615885
17.725332	1003.029012	11.620890
18.078163	998.607698	11.625895
17.968481	1004.158785	11.630899
17.997254	1024.471887	11.635904
18.402288	1028.075331	11.640909
18.252857	1030.046736	11.645914
18.304482	1042.729986	11.650919
18.588915	1026.605822	11.655923
18.494326	1011.740627	11.660928
18.380374	1013.944493	11.665933
18.326560	1013.375916	11.670938
18.400414	1032.869700	11.675943
18.316276	1038.981283	11.680947
18.365283	1027.409542	11.685952
18.735906	1036.525261	11.690957
18.477678	1036.467110	11.695962
18.613360	1034.676117	11.700967
18.523686	1034.450731	11.705971
18.752770	1027.341485	11.710976
18.914641	1023.909420	11.715981
18.502644	1020.018525	11.720986
18.856605	1026.159575	11.725991
18.982238	1035.915195	11.730995
18.700939	1019.275716	11.736000
19.186176	1042.469704	11.741005
18.874290	1035.363159	11.746010
19.082070	1022.496635	11.751015
19.215041	1035.857618	11.756019
18.787981	1033.929297	11.761024
19.166712	1036.896688	11.766029
19.043646	1041.866445	11.771034
19.699910	1052.562474	11.776039
19.263243	1050.463794	11.781043
19.475720	1053.793601	11.786048
19.640085	1049.038051	11.791053
19.726123	1054.980570	11.796058
19.887199	1053.981896	11.801063
19.744239	1054.734848	11.806067
19.722023	1039.418105	11.811072
19.816175	1033.068401	11.816077
19.566358	1030.077317	11.821082
19.764979	1049.494453	11.826087
19.693917	1056.652645	11.831091
19.857567	1057.888134	11.836096
20.014813	1055.330443	11.841101
19.956743	1062.434526	11.846106
19.922374	1060.624920	11.851111
20.022644	1062.182759	11.856115
19.868929	1055.918312	11.861120
19.820472	1052.138160	11.866125
19.583045	1057.370593	11.871130
19.869878	1048.656228	11.876135
19.765900	1065.194786	11.881139
19.789511	1076.152591	11.886144
20.377693	1080.802335	11.891149
19.909749	1088.052230	11.896154
20.457923	1084.607422	11.901159
20.169644	1095.717492	11.906163
20.199344	1079.044110	11.911168
20.730763	1081.354789	11.916173
20.498382	1088.754773	11.921178
20.847554	1078.846136	11.926183
20.758507	1088.713305	11.931187
20.903913	1083.235358	11.936192
21.006190	1076.846492	11.941197
21.067625	1075.895249	11.946202
21.029865	1073.086380	11.951207
21.060286	1094.585204	11.956211
21.292306	1073.218010	11.961216
21.420157	1078.389036	11.966221
21.071420	1076.799883	11.971226
20.988179	1070.506842	11.976231
21.003920	1086.026526	11.981235
20.985102	1081.513075	11.986240
21.564104	1079.220854	11.991245
21.222358	1086.672973	11.996250
21.260294	1084.514359	12.001255
21.230612	1085.417981	12.006259
21.461915	1082.315456	12.011264
21.279620	1073.950294	12.016269
21.319926	1080.472560	12.021274
21.531386	1082.894198	12.026279
21.443945	1073.148245	12.031283
21.219645	1074.437728	12.036288
21.396283	1075.630145	12.041293
21.053526	1084.613669	12.046298
21.792338	1090.504128	12.051303
21.762531	1092.823897	12.056307
22.009875	1080.141826	12.061312
21.823345	1072.058043	12.066317
21.475446	1083.921946	12.071322
21.795813	1079.624059	12.076327
22.024493	1080.497512	12.081331
21.790278	1072.266791	12.086336
22.074527	1071.157006	12.091341
21.738957	1066.795007	12.096346
21.650679	1057.088623	12.101351
21.711159	1053.904539	12.106355
21.678491	1048.287848	12.111360
21.756214	1033.701079	12.116365
21.662471	1040.866035	12.121370
21.572098	1045.377987	12.126375
21.689569	1056.459581	12.131379
21.493313	1050.842173	12.136384
21.794567	1044.825289	12.141389
21.668632	1049.229373	12.146394
21.978130	1046.674209	12.151399
21.486553	1038.186508	12.156403
21.529039	1021.772929	12.161408
21.468977	1015.942998	12.166413
20.999751	1027.583353	12.171418
21.168176	1046.126928	12.176423
21.351928	1036.541175	12.181427
21.381489	1061.798013	12.186432
21.829011	1041.533493	12.191437
21.675965	1051.429769	12.196442
21.820727	1042.022121	12.201447
21.394560	1044.862423	12.206451
21.572966	1031.106433	12.211456
21.632387	1022.163424	12.216461
21.209674	1032.042773	12.221466
21.386119	1029.846305	12.226471
21.416966	1033.522048	12.231475
21.462294	1049.612569	12.236480
21.555171	1056.239981	12.241485
21.656072	1056.843650	12.246490
21.828716	1027.277844	12.251495
21.115492	1044.178482	12.256499
21.066404	1024.176123	12.261504
21.464817	1031.689936	12.266509
21.465127	1050.957352	12.271514
21.806698	1050.114397	12.276519
21.955216	1044.833090	12.281523
21.623335	1044.698375	12.286528
21.649090	1034.002403	12.291533
21.473519	1027.719376	12.296538
21.567086	1025.938256	12.301543
21.558854	1031.151470	12.306547
21.286425	1025.606146	12.311552
21.604748	1025.629503	12.316557
21.120975	1033.542647	12.321562
21.625150	1026.829500	12.326567
21.381200	1029.669122	12.331571
21.450892	1024.796214	12.336576
21.828565	1034.287704	12.341581
21.462601	1024.442704	12.346586
21.786953	1026.374811	12.351591
21.585642	1030.869760	12.356595
21.559874	1031.977761	12.361600
21.830052	1019.057133	12.366605
21.524826	1016.574789	12.371610
21.956362	1029.121739	12.376615
22.148305	1024.305027	12.381619
21.820805	1021.212793	12.386624
21.545206	1008.199450	12.391629
21.267093	1007.584646	12.396634
21.151783	1005.707532	12.401639
21.208920	1008.812944	12.406643
21.494777	1012.627783	12.411648
21.955599	1012.704106	12.416653
21.263553	1024.510886	12.421658
21.332771	1012.994281	12.426663
21.691265	1017.187047	12.431667
21.444728	1010.448563	12.436672
21.566586	1008.749666	12.441677
21.432259	1012.371323	12.446682
21.358522	997.811902	12.451687
21.311356	1028.887319	12.456691
21.488031	1032.478301	12.461696
21.673058	1022.189024	12.466701
21.513162	1028.967129	12.471706
21.481843	1028.669357	12.476711
21.691758	1038.340573	12.481715
21.582020	1028.019458	12.486720
21.412873	1021.820566	12.491725
21.320936	1013.978774	12.496730
21.603414	1018.003890	12.501735
21.567532	1024.620286	12.506739
21.238570	1021.291740	12.511744
21.452362	1023.861230	12.516749
21.306957	1018.500655	12.521754
21.543217	1038.563062	12.526759
21.627068	1041.686298	12.531763
21.762544	1037.760116	12.536768
21.523596	1018.295833	12.541773
21.180524	1015.486785	12.546778
21.439927	1005.392241	12.551783
21.483743	1023.774310	12.556787
21.433414	1033.873389	12.561792
21.554379	1028.618560	12.566797
21.393085	1037.516342	12.571802
21.531354	1048.988856	12.576807
21.648172	1050.017345	12.581811
21.741903	1039.398838	12.586816
21.447983	1012.424327	12.591821
21.167351	1021.760607	12.596826
21.357385	1027.197666	12.601831
21.757952	1041.266612	12.606835
21.386942	1031.704690	12.611840
21.662711	1012.765452	12.616845
21.441187	1017.210003	12.621850
21.298203	1016.770768	12.626855
21.507691	1023.407952	12.631859
21.478764	1024.393452	12.636864
21.544793	1017.709192	12.641869
21.199847	1032.463169	12.646874
21.507965	1034.451483	12.651879
21.840846	1046.776060	12.656883
21.623586	1039.851541	12.661888
21.608756	1008.435924	12.666893
21.599347	1011.752225	12.671898
21.589396	1026.933742	12.676903
21.473016	1009.498407	12.681907
21.355539	1013.358653	12.686912
21.610178	1008.028894	12.691917
21.550908	1027.994918	12.696922
21.720137	1009.736582	12.701927
21.682799	1009.969632	12.706931
21.424947	1019.147733	12.711936
21.677276	1013.638566	12.716941
21.474882	1016.093084	12.721946
21.584223	1013.725970	12.726951
21.242071	1025.473790	12.731955
21.436789	1029.948151	12.736960
21.686697	1021.971407	12.741965
21.260184	1024.110008	12.746970
21.441817	1014.053094	12.751975
21.818444	1028.810251	12.756979
21.685279	1023.308948	12.761984
21.716494	1019.063506	12.766989
21.638771	1025.268678	12.771994
21.719813	1026.514186	12.776999
21.705279	1020.416791	12.782003
21.669226	1011.340781	12.787008
21.743553	1003.127121	12.792013
21.070243	1001.271197	12.797018
21.224479	1005.729930	12.802023
21.028693	1021.488289	12.807027
21.244551	1024.607813	12.812032
21.623470	1023.620128	12.817037
21.265460	1034.854815	12.822042
21.373252	1028.698482	12.827047
21.298324	1028.215275	12.832051
21.186884	1042.561430	12.837056
21.553223	1029.958196	12.842061
21.277257	1037.133290	12.847066
21.262360	1024.225010	12.852071
21.760671	1038.667875	12.857075
21.455096	1042.849870	12.862080
21.466057	1032.481116	12.867085
21.139360	1031.856713	12.872090
21.450110	1028.629562	12.877095
21.435075	1045.379418	12.882099
21.526761	1037.858414	12.887104
21.791832	1030.221450	12.892109
21.145977	1043.211491	12.897114
21.525307	1034.237951	12.902119
21.288641	1033.403644	12.907123
21.363597	1040.188451	12.912128
21.602339	1038.086126	12.917133
21.393492	1047.863564	12.922138
21.616815	1035.992773	12.927143
21.645728	1036.462841	12.932147
21.490878	1041.730984	12.937152
21.826545	1033.884059	12.942157
21.592612	1037.496378	12.947162
21.987302	1043.291891	12.952167
21.920998	1038.330282	12.957171
21.754434	1039.260465	12.962176
21.770626	1043.052090	12.967181
21.730676	1047.242183	12.972186
21.749031	1037.941433	12.977191
21.388591	1029.543209	12.982195
21.222448	1018.792699	12.987200
21.607731	1029.022571	12.992205
21.539093	1039.868906	12.997210
21.306908	1028.564366	13.002215
21.655710	1042.532758	13.007219
21.096316	1038.636981	13.012224
21.419882	1034.396945	13.017229
21.652127	1042.139119	13.022234
21.806711	1041.163560	13.027239
21.621325	1031.344947	13.032243
21.465799	1019.231817	13.037248
21.462136	1005.254152	13.042253
21.129116	1005.619519	13.047258
21.475615	1019.395866	13.052263
21.612873	1045.898653	13.057267
21.775569	1032.632452	13.062272
21.624602	1020.972761	13.067277
21.346656	1016.423389	13.072282
21.549186	1007.836036	13.077287
21.382351	1028.809555	13.082291
21.452391	1016.047008	13.087296
21.326225	1003.623276	13.092301
21.615804	1016.522443	13.097306
21.301018	1007.665936	13.102311
21.582678	1016.612904	13.107315
21.648793	1029.431029	13.112320
21.379578	1019.013930	13.117325
20.947738	1031.679664	13.122330
21.454810	1032.847760	13.127335
21.399557	1039.364748	13.132339
21.410272	1051.455282	13.137344
21.600352	1043.325639	13.142349
21.596795	1053.726359	13.147354
21.732320	1055.860478	13.152359
21.410720	1052.420362	13.157363
21.347149	1051.906957	13.162368
21.402512	1056.474517	13.167373
21.364450	1062.712804	13.172378
21.554429	1051.053903	13.177383
21.588721	1053.191552	13.182387
21.525689	1059.224082	13.187392
21.573455	1050.760738	13.192397
21.384944	1053.041158	13.197402
21.761684	1057.811353	13.202407
21.668883	1048.823219	13.207411
21.143614	1042.304222	13.212416
21.684109	1044.367440	13.217421
21.419762	1048.661133	13.222426
21.755671	1036.766077	13.227431
21.660602	1034.895193	13.232435
21.370346	1033.045978	13.237440
21.485391	1024.489916	13.242445
21.251177	1028.529636	13.247450
21.393166	1038.047681	13.252455
21.491580	1035.057826	13.257459
21.515735	1052.552078	13.262464
21.575421	1040.754693	13.267469
21.334983	1037.046166	13.272474
21.583372	1036.277998	13.277479
21.271880	1039.609371	13.282483
21.266286	1055.551900	13.287488
21.695619	1048.120542	13.292493
21.211471	1071.325687	13.297498
21.609496	1054.886903	13.302503
21.568280	1062.223266	13.307507
21.637279	1064.535157	13.312512
21.712986	1046.868863	13.317517
21.367754	1046.103912	13.322522
21.515741	1040.398485	13.327527
20.970384	1036.095188	13.332531
21.484636	1049.698149	13.337536
21.765904	1046.967712	13.342541
21.350987	1052.395612	13.347546
21.819831	1062.405597	13.352551
21.527773	1053.469742	13.357555
21.583885	1036.041557	13.362560
21.767264	1030.702654	13.367565
21.278103	1028.372649	13.372570
21.354897	1027.463115	13.377575
21.751158	1023.515844	13.382579
21.415015	1033.520159	13.387584
21.374969	1030.494040	13.392589
21.365948	1034.450535	13.397594
21.334899	1026.381403	13.402599
21.526146	1039.796174	13.407603
21.446093	1056.893886	13.412608
21.875460	1050.640521	13.417613
21.556173	1046.148196	13.422618
21.166596	1027.908002	13.427623
21.305276	1041.212885	13.432627
21.468379	1061.685967	13.437632
21.871837	1052.968767	13.442637
21.665359	1033.388897	13.447642
21.901376	1035.415520	13.452647
21.278348	1044.494185	13.457651
20.963652	1040.411143	13.462656
21.447160	1031.881464	13.467661
21.270007	1031.676338	13.472666
21.436074	1047.659289	13.477671
21.598026	1051.471824	13.482675
21.151084	1077.200510	13.487680
21.834103	1067.008395	13.492685
21.741428	1072.553642	13.497690
21.644060	1039.810692	13.502695
21.807617	1039.962814	13.507699
21.514078	1044.314780	13.512704
21.819319	1040.847228	13.517709
21.769982	1042.081993	13.522714
21.370108	1038.214390	13.527719
21.668585	1041.312855	13.532723
21.415316	1034.958638	13.537728
21.559314	1037.752154	13.542733
21.389366	1051.170928	13.547738
21.430792	1029.001557	13.552743
21.213550	1039.229765	13.557747
20.994505	1048.508930	13.562752
21.583872	1035.420681	13.567757
21.504623	1051.299258	13.572762
21.499512	1038.288478	13.577767
21.353662	1028.693799	13.582771
21.469760	1023.449210	13.587776
21.469957	1034.298754	13.592781
21.137095	1047.923284	13.597786
21.505045	1029.197983	13.602791
21.418295	1038.036566	13.607795
21.287678	1039.719539	13.612800
21.680019	1044.163962	13.617805
21.392742	1064.795615	13.622810
21.464779	1049.008083	13.627815
21.603878	1040.818763	13.632819
21.198875	1043.496415	13.637824
21.993246	1049.873165	13.642829
21.535405	1049.167175	13.647834
21.871458	1040.735128	13.652839
21.648282	1035.412182	13.657843
21.339292	1055.812317	13.662848
21.802454	1036.392145	13.667853
21.763901	1043.373255	13.672858
21.740237	1043.747629	13.677863
21.520954	1047.250380	13.682867
21.352376	1048.778557	13.687872
21.651634	1045.786628	13.692877
21.271443	1051.361955	13.697882
21.624437	1046.708786	13.702887
21.872242	1040.690968	13.707891
21.674374	1047.331633	13.712896
21.808989	1049.617285	13.717901
21.921206	1042.892530	13.722906
21.559429	1021.795165	13.727911
21.558694	1014.422957	13.732915
21.315977	1020.302778	13.737920
21.527560	1012.723240	13.742925
21.416581	1017.779371	13.747930
21.264477	1009.071960	13.752935
21.335098	999.110034	13.757939
21.105443	1025.691806	13.762944
21.674342	1036.255100	13.767949
21.742065	1033.139251	13.772954
21.794027	1024.454477	13.777959
21.500274	1016.859341	13.782963
21.655938	1014.246716	13.787968
21.615358	1009.575907	13.792973
21.139322	1014.354368	13.797978
21.181986	1018.529699	13.802983
21.499261	1015.233701	13.807987
21.636888	1028.906175	13.812992
21.388079	1009.659522	13.817997
21.521322	1020.158248	13.823002
21.752088	1020.323304	13.828007
21.699195	1013.448276	13.833011
21.299195	1012.226856	13.838016
21.446103	1005.703168	13.843021
21.146980	1009.926702	13.848026
21.344938	1014.400542	13.853031
21.668095	1019.370084	13.858035
21.428214	1018.498443	13.863040
21.787860	1020.946898	13.868045
21.286619	1020.966930	13.873050
21.101153	1019.861104	13.878055
21.153142	1024.632621	13.883059
21.089227	1040.592321	13.888064
21.751733	1030.804054	13.893069
21.438084	1048.446799	13.898074
21.656082	1052.005963	13.903079
21.595380	1038.557765	13.908083
21.754989	1038.557551	13.913088
21.610368	1045.505116	13.918093
21.636605	1038.986467	13.923098
21.770285	1041.461505	13.928103
21.634569	1022.646232	13.933107
21.502354	1010.797476	13.938112
21.491438	1011.489941	13.943117
21.306352	1012.262226	13.948122
21.441049	1011.967937	13.953127
21.364529	1011.442406	13.958131
21.122633	1020.986975	13.963136
21.290316	1028.386198	13.968141
21.412518	1039.662569	13.973146
21.859814	1045.508040	13.978151
21.832271	1030.900217	13.983155
21.250455	1026.618507	13.988160
21.770369	1015.692342	13.993165
21.561586	1020.464449	13.998170
21.544537	1003.454830	14.003175
21.582253	1016.354744	14.008179
21.823588	1012.777542	14.013184
21.904636	1015.240469	14.018189
21.786548	1019.029359	14.023207
21.689982	1012.457269	14.028224
21.634894	1017.697689	14.033242
21.346479	1025.201047	14.038259
21.763810	1012.285086	14.043277
21.605470	1019.755112	14.048295
21.462076	1014.371774	14.053312
21.501960	1020.136567	14.058330
21.362237	1023.877312	14.063347
21.631687	1022.063207	14.068365
21.290035	1019.659194	14.073383
21.741802	1018.210820	14.078400
21.745722	1018.494909	14.083418
21.666751	1029.324680	14.088435
21.786201	1018.568695	14.093453
21.797142	1020.454498	14.098471
21.891730	1017.993489	14.103488
21.731970	1020.271442	14.108506
21.798475	1023.642684	14.113523
21.771715	1022.679600	14.118541
21.287925	1030.019077	14.123559
21.641492	1025.593044	14.128576
21.856729	1026.365647	14.133594
21.502810	1027.861356	14.138611
21.909920	1043.895571	14.143629
21.771496	1053.010889	14.148647
21.910767	1059.955289	14.153664
22.066275	1056.985931	14.158682
22.075503	1061.467383	14.163699
22.258261	1061.271512	14.168717
21.989020	1056.856720	14.173735
22.072256	1054.460434	14.178752
22.180690	1043.261042	14.183770
21.819583	1050.749268	14.188787
22.116797	1053.379037	14.193805
22.241681	1058.867606	14.198823
21.943484	1050.592692	14.203840
21.963718	1054.309505	14.208858
21.888080	1071.103409	14.213875
22.281757	1064.656014	14.218893
22.105584	1069.771053	14.223911
21.838742	1056.825757	14.228928
21.983069	1058.556589	14.233946
21.736024	1067.020736	14.238963
22.165129	1050.955385	14.243981
22.414540	1057.474823	14.248999
21.869806	1062.908181	14.254016
22.370271	1067.234210	14.259034
21.800227	1084.089682	14.264051
22.387095	1088.460135	14.269069
22.530299	1094.342180	14.274087
22.406172	1083.019410	14.279104
22.611677	1094.867173	14.284122
22.309672	1093.584633	14.289139
22.708214	1085.887526	14.294157
22.551171	1102.405025	14.299175
22.579776	1100.781902	14.304192
22.624722	1095.206479	14.309210
22.723164	1085.683847	14.314227
22.549131	1078.987235	14.319245
22.524756	1079.305725	14.324263
22.518673	1071.492272	14.329280
22.747863	1063.366031	14.334298
22.628214	1057.495993	14.339315
22.747589	1061.541472	14.344333
22.694163	1055.695478	14.349351
22.258045	1065.459152	14.354368
22.560681	1074.560762	14.359386
22.826190	1088.513000	14.364403
22.990404	1085.817515	14.369421
22.722130	1093.397916	14.374439
22.638006	1094.899361	14.379456
23.034811	1092.283176	14.384474
22.883413	1089.232206	14.389491
22.845512	1088.014503	14.394509
22.728696	1065.612262	14.399527
22.651203	1090.112380	14.404544
22.828140	1087.721591	14.409562
22.966569	1082.480459	14.414579
22.986798	1087.428906	14.419597
23.022867	1089.183300	14.424615
22.753089	1086.803989	14.429632
22.765907	1089.516876	14.434650
22.661583	1105.712953	14.439667
23.098474	1094.989648	14.444685
23.290061	1091.210748	14.449703
22.821644	1092.383393	14.454720
22.916327	1098.347107	14.459738
22.736509	1097.968403	14.464755
22.918323	1094.307460	14.469773
23.008843	1090.668944	14.474791
22.750314	1094.499439	14.479808
22.742877	1099.752737	14.484826
23.180017	1113.130235	14.489843
23.679195	1115.741960	14.494861
23.807796	1108.257775	14.499879
23.340485	1104.080618	14.504896
23.415298	1081.402406	14.509914
23.364917	1091.749486	14.514931
23.222021	1075.816236	14.519949
23.295855	1086.443934	14.524967
22.971672	1084.491707	14.529984
23.089220	1063.156303	14.535002
22.989741	1116.072239	14.540019
23.203704	1108.986554	14.545037
23.595368	1106.819479	14.550055
23.577686	1114.131844	14.555072
23.581321	1120.967351	14.560090
23.424252	1108.149213	14.565107
23.461618	1110.387874	14.570125
23.609582	1118.850394	14.575143
23.537120	1125.935558	14.580160
23.613834	1118.736484	14.585178
23.757423	1120.365200	14.590195
23.826592	1119.702974	14.595213
23.945436	1117.211339	14.600231
23.462442	1107.421222	14.605248
23.808782	1104.163453	14.610266
23.591560	1106.601588	14.615283
23.678410	1106.076536	14.620301
23.752953	1109.509434	14.625319
23.495083	1117.236046	14.630336
24.285393	1094.877830	14.635354
23.882576	1090.894874	14.640371
23.568045	1087.778693	14.645389
23.756925	1094.221290	14.650407
23.501560	1104.272325	14.655424
23.623966	1104.949632	14.660442
23.626004	1111.757077	14.665459
24.031458	1114.401053	14.670477
24.100032	1117.087750	14.675495
23.641868	1112.512745	14.680512
24.094708	1110.675672	14.685530
23.851942	1116.321998	14.690547
23.869311	1113.365223	14.695565
24.244370	1113.104075	14.700583
24.115349	1127.551841	14.705600
24.119221	1118.118200	14.710618
24.028802	1110.796356	14.715635
24.111383	1109.395848	14.720653
24.299779	1112.900246	14.725671
24.075749	1119.532975	14.730688
24.131593	1107.237705	14.735706
24.029878	1114.583922	14.740723
24.010213	1108.988913	14.745741
24.471463	1112.770675	14.750759
24.068179	1114.389091	14.755776
24.111251	1114.102246	14.760794
24.096514	1118.175423	14.765811
23.808122	1123.188835	14.770829
24.034704	1114.120779	14.775847
23.939800	1123.386496	14.780864
24.156612	1134.018164	14.785882
24.275252	1146.523166	14.790899
24.220207	1148.024697	14.795917
24.405333	1140.573950	14.800935
24.286172	1146.202146	14.805952
24.397456	1147.821861	14.810970
24.640609	1141.799545	14.815987
24.602871	1140.333284	14.821005
24.904146	1133.147148	14.826023
24.589761	1149.389362	14.831040
24.813544	1142.118058	14.836058
24.924808	1148.664290	14.841075
24.455149	1150.486771	14.846093
24.689812	1135.297020	14.851111
24.523951	1156.604080	14.856128
24.711472	1154.092047	14.861146
24.592552	1152.011121	14.866163
24.551782	1149.019569	14.871181
24.848858	1142.076335	14.876199
24.577115	1151.235000	14.881216
25.015836	1135.300151	14.886234
25.021571	1149.970255	14.891251
24.727316	1147.951899	14.896269
24.991926	1140.018160	14.901287
24.961975	1138.992659	14.906304
24.762955	1144.447982	14.911322
25.149102	1148.199263	14.916339
24.788430	1151.344523	14.921357
25.129038	1132.296705	14.926375
24.978578	1152.300465	14.931392
24.606671	1145.542577	14.936410
25.018294	1147.411679	14.941427
24.752002	1150.758955	14.946445
25.200758	1146.547356	14.951463
25.005661	1137.489915	14.956480
25.126624	1141.580780	14.961498
25.063246	1143.469015	14.966515
24.820096	1146.022972	14.971533
25.102092	1137.449412	14.976551
25.042635	1143.187629	14.981568
25.340789	1139.508119	14.986586
24.820771	1139.296927	14.991603
24.894346	1140.527842	14.996621
24.984163	1147.747576	15.001639
25.226764	1164.593072	15.006656
25.536699	1169.990823	15.011674
25.686513	1174.431012	15.016691
25.386080	1156.068976	15.021709
25.461427	1144.822876	15.026727
24.849984	1150.947999	15.031744
25.631298	1156.920195	15.036762
25.874863	1153.947783	15.041779
25.377557	1157.264269	15.046797
25.398045	1149.581811	15.051815
25.521806	1158.001025	15.056832
25.760452	1153.914168	15.061850
25.552289	1151.189977	15.066867
25.411036	1148.673757	15.071885
25.297043	1146.470928	15.076903
25.319777	1157.415128	15.081920
25.396449	1164.968863	15.086938
25.095870	1166.412033	15.091955
25.463297	1180.168787	15.096973
25.715401	1169.154015	15.101991
25.481352	1173.828454	15.107008
25.449407	1163.584128	15.112026
25.802680	1170.637589	15.117043
26.103403	1167.964360	15.122061
26.225867	1158.766597	15.127079
26.260876	1176.815502	15.132096
25.947059	1162.818998	15.137114
26.260538	1153.057539	15.142131
26.078003	1160.459138	15.147149
26.106212	1160.662281	15.152167
25.856052	1165.265358	15.157184
25.843215	1160.340896	15.162202
25.823930	1168.858434	15.167219
25.774209	1162.292960	15.172237
25.974088	1158.194982	15.177255
25.805271	1157.051635	15.182272
25.732908	1159.089163	15.187290
25.933087	1169.224882	15.192307
25.835108	1163.563694	15.197325
25.688960	1163.568139	15.202343
26.191657	1170.654395	15.207360
26.633531	1181.774000	15.212378
26.456052	1168.051462	15.217395
26.472722	1163.704289	15.222413
26.407712	1161.945085	15.227431
26.414650	1166.224023	15.232448
26.118511	1160.935775	15.237466
26.534255	1162.687822	15.242483
26.405533	1158.319797	15.247501
26.371003	1163.008026	15.252519
26.214990	1155.927847	15.257536
26.267158	1151.650518	15.262554
26.669155	1161.993133	15.267571
26.158921	1170.203599	15.272589
26.226127	1150.486812	15.277607
26.509203	1157.416188	15.282624
26.456180	1159.526134	15.287642
26.601064	1165.316709	15.292659
26.049357	1167.825505	15.297677
26.660827	1187.580379	15.302695
26.716969	1193.194790	15.307712
27.001067	1180.218136	15.312730
27.116637	1179.019991	15.317747
26.827921	1173.497756	15.322765
26.896946	1157.143667	15.327783
26.482821	1162.938460	15.332800
26.124385	1166.361781	15.337818
26.774414	1179.099796	15.342835
26.826612	1180.898819	15.347853
26.821678	1189.701932	15.352871
26.798081	1191.289684	15.357888
26.884330	1195.348349	15.362906
27.180379	1189.968785	15.367923
27.009169	1176.537811	15.372941
27.046652	1179.824059	15.377959
27.162176	1170.128767	15.382976
26.886118	1157.666176	15.387994
27.231182	1153.908397	15.393011
27.013477	1157.068608	15.398029
27.139520	1158.361939	15.403047
26.883935	1157.720049	15.408064
26.576701	1156.999883	15.413082
27.404829	1174.065022	15.418099
27.379460	1186.902902	15.423117
27.021789	1162.236104	15.428135
27.000369	1162.972532	15.433152
27.019761	1193.669006	15.438170
27.451487	1181.002275	15.443187
27.229410	1180.995236	15.448205
27.376967	1186.411027	15.453223
27.277650	1190.118630	15.458240
27.459176	1193.024844	15.463258
27.534351	1183.265195	15.468275
27.415376	1183.710455	15.473293
27.350350	1175.854439	15.478311
27.219434	1173.585094	15.483328
27.437665	1180.852001	15.488346
27.427929	1193.259546	15.493363
27.268941	1189.461034	15.498381
27.511653	1177.994739	15.503399
27.527645	1194.259812	15.508416
27.264819	1189.900582	15.513434
27.584787	1182.552572	15.518451
27.451059	1193.111210	15.523469
27.605690	1187.809257	15.528487
27.672126	1190.065316	15.533504
27.417288	1187.065429	15.538522
27.581281	1177.370266	15.543539
27.649513	1187.921857	15.548557
27.584187	1182.968007	15.553575
27.975634	1186.045224	15.558592
27.413562	1193.233678	15.563610
27.804320	1178.994225	15.568627
27.624455	1192.138311	15.573645
27.374563	1195.108616	15.578663
27.701814	1198.757623	15.583680
28.140943	1210.373173	15.588698
27.982635	1216.558178	15.593715
28.020585	1226.480720	15.598733
28.063159	1212.262163	15.603751
28.274389	1214.227727	15.608768
28.161482	1226.285254	15.613786
28.423653	1215.937354	15.618803
28.036174	1197.263544	15.623821
27.981087	1184.139646	15.628839
28.440365	1190.929255	15.633856
28.352358	1189.739983	15.638874
28.268275	1183.829616	15.643891
27.906076	1177.035559	15.648909
28.108137	1187.996798	15.653927
28.344420	1196.064619	15.658944
28.071442	1216.876064	15.663962
28.558488	1204.850126	15.668979
28.587977	1212.905323	15.673997
28.354910	1200.171580	15.679015
28.216723	1195.454281	15.684032
28.326671	1203.999989	15.689050
28.472553	1203.386870	15.694067
28.383551	1213.496386	15.699085
28.736585	1214.803854	15.704103
28.454724	1208.681211	15.709120
28.242282	1200.194339	15.714138
28.357136	1197.634116	15.719155
28.503700	1213.123360	15.724173
28.424249	1211.210730	15.729191
28.900992	1205.004846	15.734208
28.570507	1208.908193	15.739226
28.898202	1208.217313	15.744243
28.485749	1215.139678	15.749261
28.245153	1211.366760	15.754279
28.539299	1222.338504	15.759296
28.642783	1221.095094	15.764314
28.727483	1218.936066	15.769331
28.895381	1215.565165	15.774349
28.518622	1222.261625	15.779367
28.592989	1214.951197	15.784384
28.650622	1213.411518	15.789402
28.570370	1209.038892	15.794419
28.930769	1227.339545	15.799437
29.347255	1238.996481	15.804455
29.443363	1229.345143	15.809472
28.711646	1223.061443	15.814490
29.117875	1215.987512	15.819507
28.826440	1221.921629	15.824525
28.751753	1237.270014	15.829543
29.219304	1241.321358	15.834560
29.062494	1244.012566	15.839578
29.168077	1242.035814	15.844595
28.894350	1251.739106	15.849613
29.002264	1236.440483	15.854631
29.175778	1245.369320	15.859648
29.069750	1240.884396	15.864666
29.463346	1237.040207	15.869683
29.588513	1244.559508	15.874701
29.471665	1239.332295	15.879719
29.503327	1240.422044	15.884736
29.280066	1237.308575	15.889754
29.482052	1241.042064	15.894771
29.503699	1241.395687	15.899789
29.167009	1243.683018	15.904807
29.625595	1234.392274	15.909824
29.422467	1246.061527	15.914842
29.515727	1239.501528	15.919859
29.289454	1236.055069	15.924877
29.333513	1240.394173	15.929895
29.610724	1236.637758	15.934912
29.448242	1240.577237	15.939930
29.603944	1253.238436	15.944947
29.430956	1269.425199	15.949965
29.893180	1268.088389	15.954983
30.214325	1256.518291	15.960000
30.082137	1248.828671	15.965018
29.987458	1236.939531	15.970035
29.981605	1233.671842	15.975053
29.901423	1236.536438	15.980071
29.665799	1233.793017	15.985088
29.493505	1239.135577	15.990106
29.781968	1257.499650	15.995123
29.982656	1266.872464	16.000141
29.764671	1264.330711	16.005159
30.144151	1263.518315	16.010176
30.083672	1263.458761	16.015194
30.186970	1266.169834	16.020211
30.485237	1263.561472	16.025229
30.224976	1250.408891	16.030247
30.316592	1236.548991	16.035264
29.881814	1235.674563	16.040282
30.247444	1233.815207	16.045299
30.188874	1250.446153	16.050317
29.865744	1252.992436	16.055335
30.393186	1248.315243	16.060352
30.011953	1258.111188	16.065370
30.291091	1261.229929	16.070387
30.374597	1259.656231	16.075405
30.454131	1261.655390	16.080423
30.774299	1256.463858	16.085440
30.389212	1265.977288	16.090458
30.625115	1252.596138	16.095475
30.541102	1266.162291	16.100493
30.484232	1250.841171	16.105511
30.883353	1250.871903	16.110528
30.637552	1261.097693	16.115546
30.677413	1255.886377	16.120563
30.460922	1247.407988	16.125581
30.623185	1251.355448	16.130599
30.937106	1248.285283	16.135616
30.575944	1261.941250	16.140634
30.618726	1247.408030	16.145651
30.755041	1246.606106	16.150669
30.694099	1254.590808	16.155687
30.514751	1252.259965	16.160704
30.836994	1253.717061	16.165722
30.497654	1261.236527	16.170739
30.721615	1256.157864	16.175757
30.674090	1249.933336	16.180775
30.809034	1245.089091	16.185792
30.805076	1251.191293	16.190810
30.932316	1251.899297	16.195827
30.532845	1253.830140	16.200845
30.793735	1274.806622	16.205863
31.364053	1263.923491	16.210880
31.000409	1280.113934	16.215898
31.050362	1282.868123	16.220915
31.288600	1279.415206	16.225933
31.256701	1278.890212	16.230951
31.513776	1276.272687	16.235968
31.539540	1274.061704	16.240986
31.625008	1264.621245	16.246003
31.278242	1258.910041	16.251021
31.162404	1260.718571	16.256039
31.536859	1267.524892	16.261056
31.676741	1264.992125	16.266074
31.454460	1250.595556	16.271091
31.391199	1248.630003	16.276109
30.992318	1252.113276	16.281127
31.507033	1261.829245	16.286144
31.664844	1272.523908	16.291162
31.560631	1266.509754	16.296179
31.689219	1263.952049	16.301197
31.421497	1279.238461	16.306215
31.768104	1275.607817	16.311232
31.510151	1282.211425	16.316250
31.793358	1285.288624	16.321267
31.888266	1267.665609	16.326285
31.678302	1273.775510	16.331303
31.955460	1286.019405	16.336320
32.106807	1278.355331	16.341338
31.715797	1274.806154	16.346355
31.711794	1272.408016	16.351373
31.716860	1275.852035	16.356391
32.098946	1278.443143	16.361408
32.227884	1276.582207	16.366426
32.054905	1271.939643	16.371443
31.659562	1272.507634	16.376461
31.635542	1272.286541	16.381479
31.762569	1281.886611	16.386496
31.827925	1284.559695	16.391514
31.778414	1275.224126	16.396531
32.028321	1279.796243	16.401549
31.843418	1282.207231	16.406567
32.045089	1279.079460	16.411584
31.989474	1297.352175	16.416602
32.012606	1305.247993	16.421619
32.290332	1311.736291	16.426637
32.298417	1321.622764	16.431655
32.464041	1310.689317	16.436672
32.641357	1317.536541	16.441690
32.712932	1314.459399	16.446707
32.600521	1304.952950	16.451725
32.256516	1303.622033	16.456743
32.383966	1310.134298	16.461760
32.286323	1308.853747	16.466778
32.362521	1312.236095	16.471795
32.589438	1306.354723	16.476813
32.349999	1314.281414	16.481831
32.611838	1303.224091	16.486848
32.463409	1310.346629	16.491866
32.169652	1308.771751	16.496883
32.708142	1299.608217	16.501901
32.684541	1303.648255	16.506919
32.738560	1300.242017	16.511936
32.712192	1295.009790	16.516954
32.441772	1305.810529	16.521971
32.667251	1309.453775	16.526989
32.762542	1325.524668	16.532007
33.157054	1325.205361	16.537024
33.144666	1329.391478	16.542042
32.782368	1334.965719	16.547059
33.159148	1313.776572	16.552077
32.884104	1327.911996	16.557095
33.100068	1328.835508	16.562112
33.331651	1334.247391	16.567130
33.325895	1323.489128	16.572147
33.223903	1300.642936	16.577165
33.021888	1310.616393	16.582183
33.150540	1320.205218	16.587200
33.194516	1322.225001	16.592218
32.999907	1333.218156	16.597235
33.522916	1324.259991	16.602253
33.246266	1332.258691	16.607271
33.165237	1316.819449	16.612288
33.560056	1323.381096	16.617306
33.255235	1329.998492	16.622323
33.511611	1324.774640	16.627341
33.750112	1333.169365	16.632359
33.669808	1319.079623	16.637376
33.708691	1332.488600	16.642394
33.573502	1326.891483	16.647411
33.798124	1317.146447	16.652429
33.645054	1308.041298	16.657447
33.617489	1321.758943	16.662464
33.986435	1319.787366	16.667482
33.419279	1312.607521	16.672499
33.726124	1312.925096	16.677517
33.810907	1319.212943	16.682535
34.015280	1314.445688	16.687552
33.987155	1322.890010	16.692570
33.907360	1317.821234	16.697587
33.980224	1293.206663	16.702605
33.364659	1300.620772	16.707623
33.717467	1314.530993	16.712640
34.048210	1317.809825	16.717658
33.600652	1313.023856	16.722675
33.922511	1317.523164	16.727693
33.744398	1325.554120	16.732711
34.003475	1315.013953	16.737728
33.970599	1320.865975	16.742746
33.733711	1313.905579	16.747763
34.024572	1313.963017	16.752781
33.979026	1332.890890	16.757799
34.101902	1351.232731	16.762816
34.343537	1351.209933	16.767834
34.485167	1347.256469	16.772851
34.532821	1340.032034	16.777869
34.340723	1348.441963	16.782887
34.369564	1356.256677	16.787904
34.348059	1342.432020	16.792922
34.464534	1349.663333	16.797939
34.927305	1335.284831	16.802957
34.840569	1333.387503	16.807975
34.509114	1336.289048	16.812992
34.648863	1311.930398	16.818010
34.264466	1311.812398	16.823027
34.545038	1325.012939	16.828045
34.369203	1343.054783	16.833063
34.639043	1350.481853	16.838080
34.661467	1349.660337	16.843098
34.603307	1355.875045	16.848115
35.050083	1338.802995	16.853133
34.941434	1343.177497	16.858151
34.658408	1348.592813	16.863168
34.947970	1346.948490	16.868186
34.706767	1351.419638	16.873203
34.785024	1340.668412	16.878221
34.963769	1344.131936	16.883239
35.005236	1353.626154	16.888256
35.050528	1346.307713	16.893274
34.575065	1353.196148	16.898291
34.983646	1342.585714	16.903309
34.878460	1350.281805	16.908327
34.974522	1352.945286	16.913344
35.595101	1362.636575	16.918362
35.524405	1362.139787	16.923379
35.548899	1344.716667	16.928397
35.640730	1347.673397	16.933415
35.204478	1339.212701	16.938432
35.366412	1328.978232	16.943450
35.303419	1342.515935	16.948467
35.408247	1345.363629	16.953485
35.300485	1350.842226	16.958503
35.187610	1345.707146	16.963520
35.487756	1358.630110	16.968538
35.377740	1369.971588	16.973555
35.577274	1372.538347	16.978573
35.476000	1371.859251	16.983591
35.368548	1371.970779	16.988608
35.921767	1376.008499	16.993626
35.566457	1368.536868	16.998643
35.957800	1359.568221	17.003661
36.083204	1365.514563	17.008679
35.989795	1363.932892	17.013696
35.903564	1364.940783	17.018714
35.693910	1381.586538	17.023731
36.019693	1370.355375	17.028749
35.771196	1369.964021	17.033767
35.749042	1370.585749	17.038784
35.995357	1363.475905	17.043802
35.545284	1373.506271	17.048819
35.965397	1372.357063	17.053837
35.723577	1374.088175	17.058855
35.927758	1359.823249	17.063872
36.265854	1369.106576	17.068890
36.129281	1366.827092	17.073907
36.262399	1361.086498	17.078925
36.132006	1371.474852	17.083943
36.307320	1388.708859	17.088960
36.245168	1389.955151	17.093978
36.303881	1394.128374	17.098995
36.337638	1399.390939	17.104013
36.841094	1388.254119	17.109031
36.527564	1386.021730	17.114048
36.358867	1363.867967	17.119066
36.301053	1379.349088	17.124083
36.573015	1382.344735	17.129101
36.573399	1402.675557	17.134119
36.597293	1399.626450	17.139136
36.895730	1390.663164	17.144154
36.791226	1396.098787	17.149171
36.774771	1392.982187	17.154189
36.871264	1387.651682	17.159207
36.765102	1387.031564	17.164224
36.932772	1385.246233	17.169242
37.114056	1386.091912	17.174259
36.814262	1361.821371	17.179277
36.887537	1358.621256	17.184295
36.695929	1369.955298	17.189312
37.078099	1367.545888	17.194330
36.798070	1390.444486	17.199347
37.022054	1385.346899	17.204365
37.139863	1386.890097	17.209383
37.157033	1385.460670	17.214400
36.997966	1389.107068	17.219418
37.155994	1397.036477	17.224435
37.472090	1387.022766	17.229453
37.310040	1390.292123	17.234471
37.477585	1388.698717	17.239488
37.561999	1384.532577	17.244506
37.481083	1398.294982	17.249523
37.049623	1393.581922	17.254541
37.147892	1397.800745	17.259559
36.895030	1390.555003	17.264576
37.411191	1395.668271	17.269594
37.446700	1389.708858	17.274611
37.321212	1391.441868	17.279629
37.636536	1394.839578	17.284647
37.292464	1394.814243	17.289664
37.507418	1389.935167	17.294682
37.284278	1391.512295	17.299699
37.449183	1412.279349	17.304717
37.511392	1405.035258	17.309735
37.351370	1417.473257	17.314752
37.836226	1414.938926	17.319770
37.856538	1425.885289	17.324787
37.947087	1413.648717	17.329805
38.160135	1411.659522	17.334823
38.007261	1416.937703	17.339840
38.024233	1404.791523	17.344858
37.939261	1413.683042	17.349875
37.822426	1414.544810	17.354893
38.180022	1417.547255	17.359911
37.689007	1421.053126	17.364928
37.823125	1407.678629	17.369946
37.785542	1409.643007	17.374963
37.822396	1427.352165	17.379981
38.483542	1434.355082	17.384999
37.987445	1449.229793	17.390016
38.529152	1440.125433	17.395034
38.591068	1448.015143	17.400051
38.352784	1443.158001	17.405069
38.658915	1436.007123	17.410087
38.412746	1436.976034	17.415104
38.540523	1440.554674	17.420122
38.468151	1436.474873	17.425139
38.573316	1433.920873	17.430157
38.909564	1432.549088	17.435175
38.669332	1445.331805	17.440192
38.923990	1426.813253	17.445210
38.624186	1431.930833	17.450227
38.613802	1434.303000	17.455245
38.616602	1432.613171	17.460263
38.623829	1441.353151	17.465280
38.846646	1434.355558	17.470298
38.595723	1431.510720	17.475315
38.468731	1444.088189	17.480333
38.998292	1422.788788	17.485351
38.504271	1440.636114	17.490368
39.110211	1437.034854	17.495386
38.985183	1424.601425	17.500403
38.654083	1426.949239	17.505421
39.068190	1444.708359	17.510439
39.084812	1462.469549	17.515456
39.309214	1433.487531	17.520474
39.472225	1460.800181	17.525491
39.543219	1443.920074	17.530509
39.660143	1460.271593	17.535527
39.186743	1435.855586	17.540544
39.383357	1433.063637	17.545562
39.359808	1429.677605	17.550579
39.501364	1451.551108	17.555597
39.541829	1450.324021	17.560615
39.239099	1456.200260	17.565632
39.438351	1443.290387	17.570650
39.882373	1446.329390	17.575667
39.795914	1457.472128	17.580685
39.760631	1451.055228	17.585703
39.635273	1448.913938	17.590720
39.685632	1455.954506	17.595738
40.012892	1448.620930	17.600755
39.903000	1430.391745	17.605773
39.795608	1465.905072	17.610791
39.978009	1443.031387	17.615808
40.019444	1437.887393	17.620826
39.843824	1461.713246	17.625843
39.808433	1461.580478	17.630861
40.098700	1440.523706	17.635879
39.777909	1472.538141	17.640896
39.978096	1434.955691	17.645914
40.143622	1442.545736	17.650931
39.891998	1462.792569	17.655949
40.360965	1439.055227	17.660967
39.966241	1441.095445	17.665984
40.437495	1440.822099	17.671002
39.955373	1452.874208	17.676019
40.137324	1434.353085	17.681037
40.455303	1443.531133	17.686055
40.547543	1451.993298	17.691072
40.281680	1431.385452	17.696090
40.164952	1460.235487	17.701107
39.880467	1436.015861	17.706125
40.388161	1467.441983	17.711143
40.565548	1474.198037	17.716160
40.907400	1463.121540	17.721178
40.878383	1490.052747	17.726195
40.698281	1469.256567	17.731213
41.074764	1497.515217	17.736231
40.630041	1485.947537	17.741248
40.893309	1476.423529	17.746266
40.699108	1469.645009	17.751283
40.990711	1479.616931	17.756301
41.054927	1465.663656	17.761319
41.057033	1463.800903	17.766336
40.815295	1489.875721	17.771354
41.064578	1466.042814	17.776371
40.532477	1495.059837	17.781389
40.914522	1474.496458	17.786407
40.828174	1476.899623	17.791424
40.953107	1483.568095	17.796442
41.183804	1468.309418	17.801459
40.872107	1479.197090	17.806477
41.362053	1488.555376	17.811495
41.177099	1509.384661	17.816512
41.255503	1511.881104	17.821530
41.604656	1488.519862	17.826547
41.353696	1506.531419	17.831565
41.686487	1506.737899	17.836583
41.790686	1498.305740	17.841600
41.730861	1508.262946	17.846618
41.710468	1491.524772	17.851635
41.808963	1510.097215	17.856653
41.940949	1503.631592	17.861671
42.073798	1503.203008	17.866688
41.642232	1481.488958	17.871706
41.957328	1480.351773	17.876723
41.391184	1475.257478	17.881741
42.189300	1475.510864	17.886759
41.812428	1501.904552	17.891776
41.856196	1504.244499	17.896794
41.970045	1486.088097	17.901811
42.063264	1490.619206	17.906829
42.283050	1500.465746	17.911847
41.672185	1495.801713	17.916864
41.808846	1499.389963	17.921882
42.229847	1493.252624	17.926899
41.826784	1507.919077	17.931917
42.303639	1486.928432	17.936935
41.965150	1491.890185	17.941952
42.117416	1492.644545	17.946970
42.066178	1507.953298	17.951987
41.980195	1493.890246	17.957005
42.463735	1517.858023	17.962023
42.516243	1527.764294	17.967040
42.398684	1535.836831	17.972058
42.991579	1523.873974	17.977075
42.311343	1541.073156	17.982093
42.792391	1517.406119	17.987111
42.774601	1527.326747	17.992128
43.052140	1525.564774	17.997146
42.994695	1506.208724	18.002163
42.482029	1495.974766	18.007181
43.011149	1525.555615	18.012199
42.657979	1516.035516	18.017216
43.004088	1503.412049	18.022234
42.921820	1547.373301	18.027251
42.959597	1522.065523	18.032269
43.218429	1488.667206	18.037287
42.954692	1541.947517	18.042304
42.825976	1524.079861	18.047322
43.440991	1481.053037	18.052339
43.077454	1530.081679	18.057357
43.419165	1508.211227	18.062375
42.984161	1518.629392	18.067392
43.515658	1507.889125	18.072410
43.602877	1488.461263	18.077427
43.308572	1542.764182	18.082445
42.919697	1511.444808	18.087463
43.121001	1502.780086	18.092480
43.379295	1495.902645	18.097498
43.399378	1529.232922	18.102515
43.372323	1501.778933	18.107533
43.392723	1537.077001	18.112551
43.466890	1531.304844	18.117568
43.318241	1550.983252	18.122586
43.703250	1507.577759	18.127603
43.232895	1542.178620	18.132621
43.577271	1562.786708	18.137639
43.921278	1519.076265	18.142656
43.953702	1563.086912	18.147674
44.010212	1547.344706	18.152691
43.805870	1514.303341	18.157709
43.755247	1554.385266	18.162727
43.873681	1569.679607	18.167744
44.094164	1541.750340	18.172762
44.541474	1576.555706	18.177779
44.221926	1547.913467	18.182797
44.527428	1549.080687	18.187815
44.211640	1523.310205	18.192832
44.420100	1547.874029	18.197850
44.212124	1530.130690	18.202867
43.867056	1547.501364	18.207885
44.313400	1536.027479	18.212903
44.401702	1567.597785	18.217920
44.921600	1549.956982	18.222938
44.714552	1571.203580	18.227955
44.876026	1570.252910	18.232973
44.856436	1549.849433	18.237991
44.795795	1527.989639	18.243008
44.630733	1527.240485	18.248026
44.644034	1525.553689	18.253043
44.763084	1536.243719	18.258061
44.925425	1543.772978	18.263079
44.853700	1557.068458	18.268096
44.735710	1543.757640	18.273114
45.368768	1570.111502	18.278131
44.881679	1556.609430	18.283149
45.342383	1545.417962	18.288167
45.132898	1564.234646	18.293184
44.869833	1535.699825	18.298202
45.443890	1529.036273	18.303219
45.141939	1581.452953	18.308237
45.128638	1535.606673	18.313255
45.161183	1575.761908	18.318272
45.037929	1560.631943	18.323290
45.270443	1559.770616	18.328307
45.052486	1544.905879	18.333325
45.078452	1574.219441	18.338343
45.426454	1551.393105	18.343360
45.006688	1563.196262	18.348378
45.227944	1550.012228	18.353395
45.209633	1569.290780	18.358413
45.226171	1574.941543	18.363431
45.453667	1587.803942	18.368448
45.221454	1577.400929	18.373466
45.707664	1598.565314	18.378483
45.893556	1576.533996	18.383501
45.404960	1595.915901	18.388519
45.967890	1597.547005	18.393536
46.274742	1604.019780	18.398554
46.332738	1593.373844	18.403571
46.210553	1604.777220	18.408589
46.267285	1600.942620	18.413607
46.202603	1576.634219	18.418624
46.016020	1577.886215	18.423642
46.076592	1584.146579	18.428659
46.006742	1601.946900	18.433677
45.978404	1600.917962	18.438695
46.695702	1596.353526	18.443712
46.321728	1620.786997	18.448730
46.744457	1579.001771	18.453747
46.389026	1621.856946	18.458765
46.189293	1606.309698	18.463783
46.178249	1594.992085	18.468800
46.538432	1587.989813	18.473818
46.587228	1605.970989	18.478835
46.854394	1579.541148	18.483853
46.447321	1618.624611	18.488871
46.685307	1584.991872	18.493888
46.925625	1606.585592	18.498906
46.941446	1585.166545	18.503923
46.949145	1588.295617	18.508941
46.433126	1618.619065	18.513959
46.903650	1576.642180	18.518976
46.295269	1611.027693	18.523994
46.925360	1606.389074	18.529011
47.139146	1624.114299	18.534029
47.178751	1637.661083	18.539047
47.228666	1598.861066	18.544064
47.217841	1632.504821	18.549082
47.574714	1621.952768	18.554099
47.137302	1618.860784	18.559117
47.129461	1628.397653	18.564135
47.853431	1627.199966	18.569152
47.393008	1616.125465	18.574170
47.435762	1626.124593	18.579187
47.779805	1620.323516	18.584205
47.194139	1631.302187	18.589223
47.690417	1606.621128	18.594240
47.477827	1638.705188	18.599258
47.745784	1603.735282	18.604275
47.679102	1638.767490	18.609293
47.618038	1605.305094	18.614311
47.776404	1645.792810	18.619328
47.343608	1627.136680	18.624346
47.640521	1645.002828	18.629363
47.764881	1641.530236	18.634381
48.010675	1654.831795	18.639399
48.519303	1639.597825	18.644416
48.399329	1669.683610	18.649434
48.310433	1629.423868	18.654451
48.296123	1658.555262	18.659469
48.331688	1639.048921	18.664487
48.330177	1653.684512	18.669504
48.436354	1621.452246	18.674522
48.429892	1658.279143	18.679539
48.454331	1649.510408	18.684557
48.560616	1646.495300	18.689575
48.405856	1647.267175	18.694592
48.561231	1639.651033	18.699610
48.624649	1640.377101	18.704627
48.384729	1651.435924	18.709645
48.382906	1634.715072	18.714663
49.001326	1646.552493	18.719680
48.573903	1645.455067	18.724698
49.057624	1630.014295	18.729715
48.622257	1649.523061	18.734733
48.856137	1633.135851	18.739751
48.921365	1627.446879	18.744768
48.670005	1653.389818	18.749786
49.141510	1633.198909	18.754803
48.985660	1628.276647	18.759821
48.443423	1649.344010	18.764839
49.191688	1637.055836	18.769856
48.819614	1676.961279	18.774874
49.110198	1657.903450	18.779891
49.081139	1668.983713	18.784909
49.457672	1680.066937	18.789927
49.557352	1656.455779	18.794944
49.544041	1669.383398	18.799962
49.769314	1658.693432	18.804979
49.624259	1676.587636	18.809997
49.845831	1643.349061	18.815015
49.836022	1681.574962	18.820032
49.340005	1666.885008	18.825050
50.044067	1654.246794	18.830067
49.882489	1680.038610	18.835085
49.607941	1650.522256	18.840103
49.722634	1691.081558	18.845120
49.281437	1670.452570	18.850138
49.673031	1674.632559	18.855155
49.564145	1665.881931	18.860173
49.470812	1705.793335	18.865191
50.091888	1679.336757	18.870208
49.874533	1717.410236	18.875226
49.928717	1688.058456	18.880243
50.383276	1713.137014	18.885261
50.241616	1689.160026	18.890279
50.042152	1698.903680	18.895296
50.364374	1702.915416	18.900314
50.500368	1690.389792	18.905331
50.556141	1688.008793	18.910349
50.429082	1694.550812	18.915367
50.722595	1699.215211	18.920384
50.539654	1704.732671	18.925402
50.453842	1721.006706	18.930419
50.930116	1708.289945	18.935437
50.775767	1715.780138	18.940455
51.250908	1721.920961	18.945472
51.346164	1682.978208	18.950490
51.150887	1690.047055	18.955507
51.422705	1695.756252	18.960525
50.622176	1678.469029	18.965543
51.038315	1690.760316	18.970560
51.353595	1682.034839	18.975578
51.030510	1681.984131	18.980595
51.414102	1681.156904	18.985613
51.106081	1664.401481	18.990631
51.048690	1698.822022	18.995648
50.984657	1669.854073	19.000666
50.916422	1718.255810	19.005683
51.362328	1692.792981	19.010701
51.200793	1739.326762	19.015719
51.508672	1705.089568	19.020736
51.626602	1730.953300	19.025754
51.621852	1707.649723	19.030771
51.672591	1708.000291	19.035789
51.436896	1707.753175	19.040807
51.358994	1721.834729	19.045824
51.463992	1701.184654	19.050842
51.786916	1721.277294	19.055859
52.081191	1683.169536	19.060877
51.708502	1711.754154	19.065895
52.147985	1707.043657	19.070912
52.153711	1698.471358	19.075930
51.756110	1734.196794	19.080947
52.239825	1711.436652	19.085965
52.049853	1733.725251	19.090983
52.043566	1745.803958	19.096000
51.992794	1743.262190	19.101018
52.243765	1714.453126	19.106035
52.416893	1748.500393	19.111053
52.422852	1740.799490	19.116071
52.880171	1737.226583	19.121088
52.621171	1744.129440	19.126106
52.766098	1742.555333	19.131123
52.753865	1736.710358	19.136141
52.763675	1721.952259	19.141159
52.924008	1727.641497	19.146176
52.563458	1729.261023	19.151194
52.626767	1741.172897	19.156211
52.852760	1724.503698	19.161229
52.264631	1745.300093	19.166247
52.790931	1725.352002	19.171264
52.931192	1724.728749	19.176282
52.698104	1752.356806	19.181299
53.186289	1747.312912	19.186317
53.176604	1738.831137	19.191335
53.157905	1761.145946	19.196352
53.602383	1748.876241	19.201370
53.691144	1745.484807	19.206387
53.745929	1731.137951	19.211405
53.347861	1740.630162	19.216423
53.572994	1738.731806	19.221440
53.688906	1715.015716	19.226458
53.166165	1749.361156	19.231475
53.862571	1711.629637	19.236493
53.589760	1762.714693	19.241511
53.575697	1725.363862	19.246528
53.454512	1763.400103	19.251546
53.328209	1732.066687	19.256563
53.843885	1746.583709	19.261581
53.763529	1738.673203	19.266599
53.635016	1747.412994	19.271616
53.877336	1731.716459	19.276634
54.060508	1733.409720	19.281651
54.089319	1755.968627	19.286669
53.933388	1742.591317	19.291687
54.071197	1773.841145	19.296704
54.260570	1766.139290	19.301722
54.062093	1763.359953	19.306739
54.530627	1762.388614	19.311757
54.235745	1783.254700	19.316775
54.772942	1743.133889	19.321792
54.660628	1783.643139	19.326810
54.442698	1743.004108	19.331827
54.786755	1776.383960	19.336845
54.581116	1763.642197	19.341863
54.641084	1774.497556	19.346880
54.692337	1763.053472	19.351898
54.908976	1748.320562	19.356915
55.012180	1768.342916	19.361933
54.911925	1735.490512	19.366951
54.840333	1735.111830	19.371968
55.268798	1775.268970	19.376986
54.902059	1778.909259	19.382003
55.211482	1741.119831	19.387021
54.730428	1775.955762	19.392039
55.086055	1755.080021	19.397056
55.187425	1733.810705	19.402074
54.785863	1785.317495	19.407091
55.514102	1763.026365	19.412109
55.124090	1778.667859	19.417127
55.418586	1790.429645	19.422144
55.693995	1782.143050	19.427162
55.331995	1804.309755	19.432179
55.965418	1770.206106	19.437197
55.754455	1807.152513	19.442215
56.015454	1770.504889	19.447232
55.909286	1795.580210	19.452250
55.650830	1812.666824	19.457267
55.884969	1773.868419	19.462285
55.754337	1793.162036	19.467303
55.766242	1767.883123	19.472320
55.869514	1797.598515	19.477338
55.795998	1779.320617	19.482355
55.872679	1799.133312	19.487373
55.580430	1814.779702	19.492391
56.161085	1785.949378	19.497408
56.289677	1833.616964	19.502426
56.204629	1818.121985	19.507443
56.211679	1830.804253	19.512461
56.206546	1799.511143	19.517479
56.312393	1841.241040	19.522496
56.526999	1801.434214	19.527514
56.287822	1819.914615	19.532531
56.725868	1838.217821	19.537549
56.885184	1824.643866	19.542567
56.980514	1850.479956	19.547584
57.340164	1808.826827	19.552602
56.869857	1846.955145	19.557619
56.510931	1816.715727	19.562637
56.946705	1806.630734	19.567655
57.304693	1809.120393	19.572672
57.380220	1844.149294	19.577690
57.058817	1810.921425	19.582707
57.137306	1845.133452	19.587725
57.212474	1819.493573	19.592743
56.805930	1851.605889	19.597760
57.480149	1821.810458	19.602778
56.860163	1836.977454	19.607795
57.544764	1812.262867	19.612813
57.305392	1833.485116	19.617831
57.432582	1815.945950	19.622848
57.534039	1832.498559	19.627866
57.229820	1820.978985	19.632883
57.535734	1852.175431	19.637901
57.703421	1850.405772	19.642919
57.993354	1855.622930	19.647936
58.012638	1853.442780	19.652954
57.939765	1858.675328	19.657971
57.887563	1855.847476	19.662989
58.237936	1858.860607	19.668007
57.930367	1845.068508	19.673024
58.097415	1869.977687	19.678042
58.000095	1848.588879	19.683059
58.430740	1838.937267	19.688077
58.350830	1865.848974	19.693095
58.721579	1847.786430	19.698112
58.744025	1844.487348	19.703130
58.330924	1847.351675	19.708147
58.330883	1853.640698	19.713165
58.220566	1856.840559	19.718183
58.309639	1862.775598	19.723200
58.663929	1869.649919	19.728218
58.538218	1874.137412	19.733235
58.782049	1887.996356	19.738253
58.789912	1876.186292	19.743271
58.815972	1879.655421	19.748288
59.254170	1869.582582	19.753306
59.103240	1885.346511	19.758323
59.270932	1879.897504	19.763341
59.123340	1883.257474	19.768359
59.406206	1874.702221	19.773376
59.534899	1863.458068	19.778394
59.138718	1890.878015	19.783411
59.491947	1876.102743	19.788429
59.593360	1863.341811	19.793447
59.353754	1882.464160	19.798464
59.702291	1874.799787	19.803482
59.598168	1884.528359	19.808499
59.550772	1885.437282	19.813517
59.700089	1877.224226	19.818535
58.911047	1882.854146	19.823552
59.846102	1877.795572	19.828570
59.493457	1909.032673	19.833587
59.747646	1916.994224	19.838605
59.587072	1917.985693	19.843623
59.282735	1912.759821	19.848640
60.097209	1910.432395	19.853658
59.812620	1918.132228	19.858675
60.038071	1943.927283	19.863693
60.275117	1915.426786	19.868711
60.598545	1928.669026	19.873728
60.387876	1929.655900	19.878746
60.441654	1940.098659	19.883763
60.587315	1916.615027	19.888781
60.543216	1933.340404	19.893799
60.732955	1923.873450	19.898816
60.622576	1912.472328	19.903834
60.854313	1937.316250	19.908851
60.605350	1924.090464	19.913869
60.740737	1933.312104	19.918887
60.794979	1935.707080	19.923904
61.027606	1915.129156	19.928922
61.162495	1923.882102	19.933939
61.299194	1918.873758	19.938957
61.265376	1921.246595	19.943975
61.255216	1923.277456	19.948992
61.472485	1901.482890	19.954010
61.327433	1916.906137	19.959027
61.453014	1911.605409	19.964045
61.621942	1921.428888	19.969063
61.256240	1898.986394	19.974080
61.499028	1907.086613	19.979098
61.563420	1919.813298	19.984115
61.491568	1895.337190	19.989133
61.407319	1938.615671	19.994151
61.629495	1924.078331	19.999168
61.902770	1941.081869	20.004186
61.618193	1947.532716	20.009203
61.765911	1929.502494	20.014221
62.296854	1952.772870	20.019239
62.233254	1935.381967	20.024256
62.049662	1924.720832	20.029274
62.205857	1952.614380	20.034291
62.260976	1941.438530	20.039309
62.366723	1925.788736	20.044327
62.133989	1940.612504	20.049344
62.458874	1919.823229	20.054362
62.371351	1935.004511	20.059379
62.058387	1936.717144	20.064397
62.545779	1945.171637	20.069415
62.867217	1956.540719	20.074432
62.761598	1955.066324	20.079450
62.764231	1979.339658	20.084467
62.417032	1949.669109	20.089485
63.151710	1966.658868	20.094503
62.811062	1973.584292	20.099520
63.198143	1952.832243	20.104538
63.212822	1960.078524	20.109555
63.360366	1964.354151	20.114573
63.218614	1964.979247	20.119591
63.082192	1969.773650	20.124608
63.567412	1960.711014	20.129626
63.594754	1962.238815	20.134643
63.548007	1952.367530	20.139661
63.376134	1950.883252	20.144679
63.290987	1960.015809	20.149696
63.376915	1963.376308	20.154714
63.369934	1934.880083	20.159731
63.020722	1975.594392	20.164749
63.470847	1962.162697	20.169767
63.720890	1982.541035	20.174784
63.744827	1991.676665	20.179802
63.503699	1995.952937	20.184819
63.918063	1991.409955	20.189837
63.961162	1977.632591	20.194855
63.810121	1981.314036	20.199872
64.132572	1986.255491	20.204890
64.260737	1986.835968	20.209907
64.074128	1978.294178	20.214925
64.388723	2008.607094	20.219943
64.520153	1999.344449	20.224960
64.639281	2009.946727	20.229978
64.886440	2005.312427	20.234995
64.781090	1996.081254	20.240013
64.741031	2009.132994	20.245031
64.882977	2013.321436	20.250048
64.574343	2003.567389	20.255066
64.837213	2008.186439	20.260083
64.632295	1994.325915	20.265101
64.989287	1997.133524	20.270119
64.978275	2000.454435	20.275136
65.292098	1989.089423	20.280154
65.233847	1992.974727	20.285171
65.097781	1998.450215	20.290189
65.090272	1985.445419	20.295207
64.993141	1999.266036	20.300224
64.983230	2000.919335	20.305242
65.020675	2016.524372	20.310259
64.944450	2024.379799	20.315277
65.282921	2043.007465	20.320295
65.695258	2029.300157	20.325312
65.688383	2023.904106	20.330330
65.541907	2036.581151	20.335347
66.031450	2050.368030	20.340365
66.439377	2038.446840	20.345383
66.231166	2034.470331	20.350400
66.178091	2031.736967	20.355418
66.519913	2015.907852	20.360435
66.366450	2022.029503	20.365453
66.487129	2008.244457	20.370471
66.321540	2019.271254	20.375488
66.525818	2003.704765	20.380506
66.489439	2028.321037	20.385523
66.338587	1998.653681	20.390541
66.704987	2023.943473	20.395559
66.327223	2000.164074	20.400576
66.310159	2020.001460	20.405594
66.592644	2025.514029	20.410611
66.708930	2041.649226	20.415629
66.866919	2033.776053	20.420647
66.806619	2055.456141	20.425664
67.083703	2043.444127	20.430682
66.875521	2035.747329	20.435699
66.997365	2053.256505	20.440717
67.056771	2027.017864	20.445735
66.934227	2043.836105	20.450752
67.025616	2042.597701	20.455770
67.140644	2047.172700	20.460787
67.140185	2032.055693	20.465805
67.560074	2049.765875	20.470823
67.591543	2084.221924	20.475840
67.738178	2066.618005	20.480858
67.933741	2066.707954	20.485875
67.723497	2103.763541	20.490893
68.197999	2060.768427	20.495911
67.879599	2091.509663	20.500928
68.134349	2075.384476	20.505946
68.103794	2069.136438	20.510963
68.030581	2066.305603	20.515981
67.854147	2070.497645	20.520999
67.912582	2076.340128	20.526016
67.682310	2070.278101	20.531034
67.986233	2073.923192	20.536051
67.852883	2072.830742	20.541069
68.008328	2071.262789	20.546087
67.995657	2113.828791	20.551104
68.199190	2106.741141	20.556122
68.482586	2098.637143	20.561139
68.360749	2109.483994	20.566157
68.609473	2098.816709	20.571175
68.773237	2151.987034	20.576192
69.079282	2127.933200	20.581210
69.137350	2115.965493	20.586227
69.074031	2150.789182	20.591245
69.451978	2114.520029	20.596263
69.503908	2135.115798	20.601280
69.481888	2126.955096	20.606298
69.308842	2111.319675	20.611315
69.307196	2140.852723	20.616333
69.604183	2123.179140	20.621351
69.304434	2128.105037	20.626368
69.673402	2128.703749	20.631386
69.766188	2124.128639	20.636403
69.277321	2115.627105	20.641421
69.411498	2136.491339	20.646439
69.902013	2116.993601	20.651456
69.367171	2145.093681	20.656474
69.565448	2109.241742	20.661491
69.739549	2154.096775	20.666509
70.110250	2145.950513	20.671527
69.962972	2163.507459	20.676544
70.184478	2154.905199	20.681562
70.519018	2141.554696	20.686579
69.910587	2156.262414	20.691597
70.593790	2150.910425	20.696615
70.529363	2159.251694	20.701632
70.543909	2139.765336	20.706650
70.398198	2164.743777	20.711667
70.573064	2147.223351	20.716685
70.491260	2130.469064	20.721703
70.413920	2165.722900	20.726720
70.447760	2161.080098	20.731738
70.811267	2179.752714	20.736755
70.821505	2172.916089	20.741773
70.918843	2172.463262	20.746791
71.057728	2183.749163	20.751808
71.137163	2178.590195	20.756826
70.910193	2180.986013	20.761843
71.298148	2188.329400	20.766861
71.544518	2171.443289	20.771879
71.843370	2208.496607	20.776896
71.743736	2177.128088	20.781914
71.637870	2167.445415	20.786931
71.501718	2190.182320	20.791949
72.007159	2182.363773	20.796967
72.319636	2176.736619	20.801984
71.639350	2204.800231	20.807002
72.101345	2175.877947	20.812019
72.001411	2179.246901	20.817037
72.318118	2185.576006	20.822055
72.503968	2186.924392	20.827072
72.475685	2189.476507	20.832090
72.546172	2194.203379	20.837107
72.227001	2185.692044	20.842125
72.253521	2209.283172	20.847143
72.654121	2184.006044	20.852160
72.409982	2194.045025	20.857178
72.544641	2193.370735	20.862195
72.425908	2184.816424	20.867213
72.630289	2187.474585	20.872231
72.362100	2193.546961	20.877248
72.586314	2207.783732	20.882266
73.211903	2213.834708	20.887283
73.165821	2212.745633	20.892301
73.132381	2220.661198	20.897319
73.128411	2208.414648	20.902336
73.025977	2226.589030	20.907354
73.314815	2204.132917	20.912371
72.923980	2220.943023	20.917389
73.277362	2217.010614	20.922407
73.292370	2200.498005	20.927424
73.137454	2244.315646	20.932442
73.871372	2234.389674	20.937459
73.490273	2249.913054	20.942477
73.806354	2241.279143	20.947495
74.027832	2241.299678	20.952512
73.716069	2263.188497	20.957530
73.948518	2226.995752	20.962547
73.770185	2238.951291	20.967565
73.752265	2246.616634	20.972583
73.902120	2240.061317	20.977600
74.153636	2265.585364	20.982618
74.593079	2251.255306	20.987635
74.428205	2267.305025	20.992653
74.501747	2283.321460	20.997671
74.877979	2252.122291	21.002688
74.469174	2293.702748	21.007706
74.859121	2269.883848	21.012723
74.798598	2271.082762	21.017741
74.660122	2269.173896	21.022759
74.949016	2258.883135	21.027776
74.707875	2275.392568	21.032794
75.178136	2264.572638	21.037811
74.988813	2253.995548	21.042829
75.005915	2282.062927	21.047847
75.178667	2271.428083	21.052864
75.050006	2290.156520	21.057882
75.432643	2272.518649	21.062899
75.423212	2273.443564	21.067917
75.389163	2272.486278	21.072935
75.640268	2282.720057	21.077952
75.409843	2280.543485	21.082970
75.935764	2263.757409	21.087987
75.980694	2299.863559	21.093005
76.513918	2298.953451	21.098023
76.421098	2274.395100	21.103040
76.034929	2265.754398	21.108058
76.230158	2255.349583	21.113075
76.233144	2265.623706	21.118093
76.117586	2288.985141	21.123111
76.152245	2294.124402	21.128128
76.170945	2286.711411	21.133146
76.543894	2297.224655	21.138163
76.650140	2299.200823	21.143181
76.533895	2305.237216	21.148199
76.753846	2297.781900	21.153216
76.668125	2297.976486	21.158234
76.561041	2291.356725	21.163251
76.952609	2306.722337	21.168269
76.947099	2323.745614	21.173287
77.322225	2321.168860	21.178304
76.967332	2333.705573	21.183322
77.503596	2308.604804	21.188339
77.269641	2326.463645	21.193357
77.170491	2321.292206	21.198375
77.300976	2301.235775	21.203392
77.055559	2321.768326	21.208410
77.496867	2298.505927	21.213427
77.288242	2347.780044	21.218445
77.797485	2339.132575	21.223463
77.783308	2327.658367	21.228480
77.702383	2354.868455	21.233498
78.425259	2340.895821	21.238515
77.874838	2358.262452	21.243533
78.251672	2332.287258	21.248551
78.323349	2347.459312	21.253568
78.256661	2342.078187	21.258586
78.194462	2333.569831	21.263603
78.568830	2327.249242	21.268621
78.142848	2351.983252	21.273639
78.498840	2322.077883	21.278656
78.218586	2367.230198	21.283674
78.836047	2357.474520	21.288691
78.937809	2389.511678	21.293709
78.746469	2358.717413	21.298727
78.919752	2388.916016	21.303744
78.616311	2367.567965	21.308762
79.266791	2345.745337	21.313779
79.034201	2383.572868	21.318797
79.246623	2353.246718	21.323815
79.103136	2384.638680	21.328832
79.063315	2371.610376	21.333850
79.570259	2379.925936	21.338867
79.283485	2396.994941	21.343885
79.833234	2399.229959	21.348903
79.958248	2380.120510	21.353920
79.665236	2388.271838	21.358938
79.883221	2381.354792	21.363955
80.125069	2381.140048	21.368973
80.167011	2372.795967	21.373991
80.330549	2384.703398	21.379008
79.709636	2393.764357	21.384026
80.224951	2390.625663	21.389043
80.279317	2387.947459	21.394061
80.482500	2405.908939	21.399079
80.740059	2391.685618	21.404096
80.528227	2422.547416	21.409114
80.665109	2407.496996	21.414131
80.825975	2401.413353	21.419149
80.583153	2418.005016	21.424167
80.937031	2386.414277	21.429184
80.505229	2412.608364	21.434202
80.879596	2409.973511	21.439219
80.808759	2397.407901	21.444237
80.818241	2438.246419	21.449255
81.363982	2439.218097	21.454272
80.993754	2430.891733	21.459290
81.123503	2445.016382	21.464307
81.281135	2425.466709	21.469325
81.260768	2433.165576	21.474343
81.641535	2448.999486	21.479360
81.420944	2444.150979	21.484378
82.094112	2451.646443	21.489395
82.309656	2464.352648	21.494413
82.187298	2458.827766	21.499431
82.127358	2430.973761	21.504448
82.564610	2449.392708	21.509466
82.422209	2441.173158	21.514483
82.824308	2413.671815	21.519501
82.464483	2432.432579	21.524519
82.500315	2392.939736	21.529536
82.077767	2432.044365	21.534554
82.126438	2412.282413	21.539571
82.132261	2448.869459	21.544589
82.263653	2455.608927	21.549607
82.578210	2448.092828	21.554624
82.618824	2455.232183	21.559642
82.771476	2461.597011	21.564659
83.184174	2476.813136	21.569677
83.005645	2482.924819	21.574695
83.490696	2479.130228	21.579712
83.386448	2480.449395	21.584730
83.043906	2470.572230	21.589747
83.336388	2489.159039	21.594765
82.954164	2489.201914	21.599783
83.331295	2476.268267	21.604800
83.379958	2496.927208	21.609818
83.539272	2516.464209	21.614835
83.789159	2512.650480	21.619853
83.896270	2515.773337	21.624871
83.989441	2502.059068	21.629888
84.312105	2510.428476	21.634906
83.835361	2506.738490	21.639923
83.890251	2521.636536	21.644941
84.468676	2519.639268	21.649959
84.322981	2540.898732	21.654976
84.638616	2541.551590	21.659994
84.940043	2520.875319	21.665011
84.808674	2535.121925	21.670029
84.789522	2529.958104	21.675047
85.114432	2536.151555	21.680064
85.314460	2539.313872	21.685082
85.211758	2526.043759	21.690099
85.190062	2524.734469	21.695117
85.087808	2529.152352	21.700135
85.304971	2527.167860	21.705152
85.278630	2509.631106	21.710170
85.426963	2543.361707	21.715187
85.360856	2512.605350	21.720205
85.317805	2533.855514	21.725223
85.694821	2518.654994	21.730240
85.266914	2525.455371	21.735258
85.578852	2550.080690	21.740275
85.795003	2547.182378	21.745293
85.920669	2546.684909	21.750311
86.172810	2543.136669	21.755328
86.209808	2554.531920	21.760346
86.049927	2554.424500	21.765363
86.016974	2542.006889	21.770381
86.077472	2534.938696	21.775399
86.250226	2564.731887	21.780416
86.166909	2555.152331	21.785434
86.278084	2586.407370	21.790451
86.631107	2580.625724	21.795469
86.638111	2565.219092	21.800487
86.554588	2601.258380	21.805504
86.711384	2568.289949	21.810522
87.082569	2583.972157	21.815539
87.354716	2612.567397	21.820557
87.458812	2598.221261	21.825575
87.707088	2585.837421	21.830592
87.470691	2596.349737	21.835610
87.308081	2580.781363	21.840627
87.593192	2598.306061	21.845645
87.562083	2606.359111	21.850663
87.658264	2588.086955	21.855680
87.365712	2610.209984	21.860698
87.389352	2598.986736	21.865715
87.535111	2602.335484	21.870733
87.571454	2625.744812	21.875751
87.764020	2625.523767	21.880768
88.297550	2620.550221	21.885786
88.076055	2639.095697	21.890803
88.527462	2627.526555	21.895821
88.493785	2621.103375	21.900839
88.721676	2607.771815	21.905856
88.593176	2636.034567	21.910874
88.864210	2629.582455	21.915891
89.299968	2633.157114	21.920909
89.160246	2619.641906	21.925927
89.033534	2639.072879	21.930944
89.358486	2606.034285	21.935962
88.886911	2617.750588	21.940979
89.357125	2631.570999	21.945997
89.019491	2647.297093	21.951015
89.064302	2630.937342	21.956032
89.324314	2648.534534	21.961050
89.014949	2648.368361	21.966067
89.567022	2652.045607	21.971085
89.614948	2649.334561	21.976103
89.852494	2687.502426	21.981120
90.064387	2656.778515	21.986138
90.006629	2661.124057	21.991155
90.126034	2677.467115	21.996173
90.132568	2665.222439	22.001191
90.047794	2654.172177	22.006208
90.037260	2671.460948	22.011226
90.042704	2691.482075	22.016243
90.383767	2680.569179	22.021261
90.383441	2682.393284	22.026279
91.018126	2690.712252	22.031296
90.918396	2687.627530	22.036314
90.676234	2708.089314	22.041331
91.059793	2694.021010	22.046349
90.964489	2690.351164	22.051367
91.132004	2686.458498	22.056384
91.422224	2679.111341	22.061402
90.814021	2699.449002	22.066419
91.254297	2697.410817	22.071437
91.146555	2705.239387	22.076455
91.591068	2707.805865	22.081472
91.869473	2719.585921	22.086490
92.013220	2713.743995	22.091507
92.059537	2712.248438	22.096525
91.815646	2720.632805	22.101543
91.988347	2715.005713	22.106560
92.068144	2694.621747	22.111578
91.882564	2716.296054	22.116595
92.032125	2712.668171	22.121613
92.004076	2692.815819	22.126631
92.165344	2751.047919	22.131648
92.389108	2720.711331	22.136666
92.458176	2741.073976	22.141683
92.722509	2725.195887	22.146701
92.644738	2743.942747	22.151719
92.798299	2725.681719	22.156736
93.211550	2764.602041	22.161754
93.098800	2756.749631	22.166771
93.302014	2779.593797	22.171789
93.066138	2756.237299	22.176807
93.179807	2780.051426	22.181824
93.518010	2740.420540	22.186842
93.123125	2776.745884	22.191859
93.459149	2757.560604	22.196877
93.344512	2774.609677	22.201895
93.663598	2776.190148	22.206912
94.162021	2775.462544	22.211930
93.950586	2798.344546	22.216947
94.717677	2782.420044	22.221965
94.825506	2762.427157	22.226983
94.865774	2793.365163	22.232000
94.972879	2741.403892	22.237018
94.622676	2755.334014	22.242035
94.741750	2746.467723	22.247053
94.749903	2744.015490	22.252071
94.573008	2728.033928	22.257088
95.240084	2733.843329	22.262106
95.077494	2732.923815	22.267123
94.961659	2733.417384	22.272141
95.080874	2754.953475	22.277159
95.068926	2757.241158	22.282176
95.018262	2774.103051	22.287194
95.129584	2784.331161	22.292211
95.207528	2763.082168	22.297229
94.988034	2763.883299	22.302247
95.233855	2790.755785	22.307264
95.899387	2795.235368	22.312282
95.471149	2789.015043	22.317299
95.754696	2804.038162	22.322317
95.813415	2804.572329	22.327335
95.797395	2800.783625	22.332352
95.957279	2786.417396	22.337370
95.969197	2810.102283	22.342387
95.899967	2803.659521	22.347405
95.600572	2852.043687	22.352423
95.853956	2823.372058	22.357440
95.939982	2862.132449	22.362458
96.256621	2857.633893	22.367475
96.682982	2847.316865	22.372493
96.863122	2857.370445	22.377511
96.938987	2866.216751	22.382528
96.945840	2846.140743	22.387546
96.946777	2887.687440	22.392563
97.545130	2884.974313	22.397581
97.665541	2864.290241	22.402599
98.156163	2868.056787	22.407616
98.186490	2867.524171	22.412634
97.855104	2850.480852	22.417651
97.815454	2837.182308	22.422669
98.236075	2856.388639	22.427687
98.137905	2848.481940	22.432704
98.121542	2853.783703	22.437722
98.137212	2857.087970	22.442739
98.261189	2865.291838	22.447757
98.665319	2862.949486	22.452775
98.180888	2852.456773	22.457792
98.611364	2861.632736	22.462810
98.071971	2870.734471	22.467827
98.588483	2858.545959	22.472845
98.548742	2864.978614	22.477863
98.842603	2880.306931	22.482880
98.898200	2879.449362	22.487898
98.880814	2892.424340	22.492915
99.051186	2889.117164	22.497933
98.822143	2895.804194	22.502951
98.904729	2900.589933	22.507968
99.259408	2902.149012	22.512986
99.201437	2914.159846	22.518003
99.509294	2929.101347	22.523021
99.511248	2927.470472	22.528039
99.385462	2916.092256	22.533056
99.819019	2947.547580	22.538074
100.102630	2946.569483	22.543091
100.219671	2945.689527	22.548109
100.400571	2955.824858	22.553127
100.451289	2952.562705	22.558144
100.816886	2952.281028	22.563162
100.235790	2935.155509	22.568179
100.493783	2968.094043	22.573197
100.608297	2934.304832	22.578215
100.292009	2962.956842	22.583232
100.877949	2961.929747	22.588250
100.928598	2975.919649	22.593267
100.906686	2976.158341	22.598285
100.728676	2982.670518	22.603303
100.967664	2961.129692	22.608320
101.177376	2987.620516	22.613338
101.370771	2977.600906	22.618355
101.386467	3017.606283	22.623373
102.235620	2997.431147	22.628391
101.772638	2993.608265	22.633408
101.837324	2998.577018	22.638426
101.924334	3004.011016	22.643443
101.894186	2997.133249	22.648461
102.227136	2994.885606	22.653479
102.114723	3004.879751	22.658496
102.453451	2993.879685	22.663514
102.125043	2996.800725	22.668531
102.547717	3003.121947	22.673549
102.462458	3028.307749	22.678567
102.362625	3016.791597	22.683584
102.410890	3013.573870	22.688602
102.498776	3031.154140	22.693619
102.858574	3037.217965	22.698637
102.987681	3037.654392	22.703655
102.698761	3034.630442	22.708672
103.428127	3047.775154	22.713690
103.424676	3053.107967	22.718707
103.453802	3048.272136	22.723725
103.836448	3067.484802	22.728743
103.944922	3056.322401	22.733760
104.182828	3051.124483	22.738778
104.144876	3076.890404	22.743795
104.335467	3061.328118	22.748813
104.661927	3055.452201	22.753831
104.558519	3051.799288	22.758848
104.689228	3062.059111	22.763866
104.681843	3058.656749	22.768883
104.747784	3049.477821	22.773901
104.867570	3054.243520	22.778919
104.730881	3045.904729	22.783936
104.815059	3060.531218	22.788954
104.871906	3052.885218	22.793971
105.161504	3050.200846	22.798989
104.938605	3045.112595	22.804007
104.932057	3052.688452	22.809024
105.116486	3059.936530	22.814042
105.371408	3077.949586	22.819059
105.171789	3095.150237	22.824077
105.316380	3090.500491	22.829095
105.351983	3104.019390	22.834112
105.832901	3105.390033	22.839130
105.606617	3114.001499	22.844147
105.434022	3114.749547	22.849165
106.000223	3127.745729	22.854183
105.712745	3151.917828	22.859200
106.470296	3139.530184	22.864218
106.343938	3152.276567	22.869235
106.593437	3136.869991	22.874253
107.071801	3133.543538	22.879271
106.824912	3132.956008	22.884288
106.997808	3131.963305	22.889306
106.677196	3141.425186	22.894323
107.110796	3139.786809	22.899341
107.273997	3147.360818	22.904359
107.082902	3176.136440	22.909376
107.529651	3155.803438	22.914394
107.259084	3166.595344	22.919411
107.206912	3157.568117	22.924429
107.482840	3159.681743	22.929447
107.690259	3187.214741	22.934464
108.011137	3183.684492	22.939482
107.711142	3185.176522	22.944499
108.157493	3202.190126	22.949517
108.282853	3183.818180	22.954535
108.357343	3181.286075	22.959552
108.568169	3190.186570	22.964570
109.022027	3168.887268	22.969587
108.401623	3178.194825	22.974605
109.129265	3198.899876	22.979623
108.991941	3191.516025	22.984640
108.858670	3220.856726	22.989658
109.177340	3187.608587	22.994675
109.194044	3222.416571	22.999693
109.361900	3187.424221	23.004711
108.949032	3223.983227	23.009728
109.570633	3211.850819	23.014746
109.505234	3202.042227	23.019763
109.777470	3229.352590	23.024781
109.734023	3240.171260	23.029799
109.833444	3229.259521	23.034816
109.819563	3222.227241	23.039834
110.074618	3251.076601	23.044851
109.895187	3236.452546	23.049869
110.647483	3235.738717	23.054887
110.721520	3265.738654	23.059904
110.892216	3257.062831	23.064922
111.206607	3260.925233	23.069939
111.192975	3260.863704	23.074957
111.032394	3249.521452	23.079975
110.897872	3258.709890	23.084992
111.078267	3265.958714	23.090010
110.704240	3246.109650	23.095027
110.561740	3277.184017	23.100045
111.601748	3259.418899	23.105063
111.250718	3274.535043	23.110080
111.225511	3292.010165	23.115098
111.846713	3267.027149	23.120115
111.415381	3303.380850	23.125133
112.160406	3284.302713	23.130151
112.066957	3304.743189	23.135168
112.054090	3305.971557	23.140186
112.497453	3307.939731	23.145203
112.700218	3300.895679	23.150221
112.670705	3299.175388	23.155239
112.481059	3320.845733	23.160256
112.321754	3296.543251	23.165274
112.668504	3322.418952	23.170291
112.552949	3308.991281	23.175309
112.418393	3308.429879	23.180327
112.950948	3346.731776	23.185344
112.949686	3325.476504	23.190362
113.197338	3337.382316	23.195379
113.463734	3356.408600	23.200397
113.769371	3341.698439	23.205415
113.581245	3376.984668	23.210432
113.996769	3332.957692	23.215450
113.943959	3362.860065	23.220467
113.814279	3347.561715	23.225485
114.136369	3353.241534	23.230503
113.960501	3361.381011	23.235520
114.442664	3360.913197	23.240538
114.600745	3393.405317	23.245555
114.513526	3376.235132	23.250573
114.785155	3373.862702	23.255591
114.684715	3387.745730	23.260608
114.579503	3389.263354	23.265626
114.904237	3383.592886	23.270643
115.062069	3394.417332	23.275661
115.292445	3401.884796	23.280679
115.213752	3413.438395	23.285696
115.330333	3387.554747	23.290714
115.518887	3421.646739	23.295731
115.595211	3400.418316	23.300749
115.773914	3437.187151	23.305767
116.091845	3414.882650	23.310784
115.992072	3449.800995	23.315802
116.404176	3421.989388	23.320819
116.202299	3426.663340	23.325837
116.457742	3430.448662	23.330855
116.313307	3441.175033	23.335872
116.427663	3418.664646	23.340890
116.697629	3458.013200	23.345907
116.586478	3451.379398	23.350925
116.911209	3448.170195	23.355943
116.743919	3464.128793	23.360960
116.861560	3446.440522	23.365978
117.016389	3456.920174	23.370995
117.340795	3483.599702	23.376013
117.545607	3463.665907	23.381031
117.390636	3478.105979	23.386048
117.447994	3485.616808	23.391066
117.800012	3492.508791	23.396083
117.752987	3503.846601	23.401101
118.291928	3500.662224	23.406119
118.565514	3497.786034	23.411136
118.483342	3503.584651	23.416154
118.674908	3496.373957	23.421171
118.348424	3504.892291	23.426189
118.572261	3479.406706	23.431207
118.288259	3500.722657	23.436224
118.956303	3532.199279	23.441242
119.056583	3527.345650	23.446259
118.979005	3528.632339	23.451277
119.222000	3526.790694	23.456295
119.286961	3520.332510	23.461312
119.365015	3523.431900	23.466330
119.624518	3518.626040	23.471347
119.579473	3528.188177	23.476365
120.112084	3538.278844	23.481383
120.299054	3553.959227	23.486400
120.101110	3550.215856	23.491418
120.184871	3545.895031	23.496435
120.097038	3549.245063	23.501453
120.305542	3555.570789	23.506471
120.322902	3553.868952	23.511488
120.105065	3556.993507	23.516506
120.601963	3563.631158	23.521523
120.363971	3587.494812	23.526541
120.852522	3567.585640	23.531559
120.584975	3587.233836	23.536576
121.260145	3589.559967	23.541594
121.205230	3612.850920	23.546611
120.999332	3596.659069	23.551629
121.324049	3605.736738	23.556647
121.792405	3623.780152	23.561664
121.973004	3627.069307	23.566682
122.365725	3632.328934	23.571699
122.388068	3627.976974	23.576717
122.677106	3640.898249	23.581735
122.524580	3639.376881	23.586752
122.169517	3631.162249	23.591770
122.337365	3626.824846	23.596787
122.255111	3637.642918	23.601805
122.414047	3639.459839	23.606823
122.592774	3652.936760	23.611840
122.864395	3665.301549	23.616858
123.191127	3656.633649	23.621875
122.907433	3652.970787	23.626893
123.136116	3667.925673	23.631911
123.342484	3683.618835	23.636928
123.205724	3694.953796	23.641946
123.974754	3687.377186	23.646963
123.611775	3694.825355	23.651981
123.653940	3691.062539	23.656999
123.989142	3687.937357	23.662016
123.643035	3715.142706	23.667034
124.326408	3716.088607	23.672051
124.347920	3721.570288	23.677069
124.831256	3720.609854	23.682087
124.825063	3739.897212	23.687104
124.869226	3745.355624	23.692122
125.372358	3731.552021	23.697139
125.310970	3737.701395	23.702157
125.456919	3732.252811	23.707175
125.490083	3734.778879	23.712192
125.109972	3742.456350	23.717210
125.742214	3731.467143	23.722227
125.690764	3733.581141	23.727245
125.704187	3730.496246	23.732263
125.504044	3725.172073	23.737280
125.136003	3754.982347	23.742298
125.753050	3751.092451	23.747315
126.152579	3759.528203	23.752333
126.098564	3764.304544	23.757351
126.092168	3769.199152	23.762368
126.277536	3787.321718	23.767386
126.721250	3794.957529	23.772403
126.812514	3800.098522	23.777421
126.869733	3791.902227	23.782439
127.252942	3778.523600	23.787456
126.547371	3813.845405	23.792474
127.116120	3796.175244	23.797491
127.010689	3810.258483	23.802509
127.295786	3823.043676	23.807527
127.535003	3818.374680	23.812544
127.615314	3854.810206	23.817562
127.909450	3825.728152	23.822579
127.807193	3857.049838	23.827597
127.870006	3858.752321	23.832615
128.182521	3865.520988	23.837632
128.368074	3861.317566	23.842650
128.349108	3870.558757	23.847667
128.597928	3888.092372	23.852685
128.892049	3900.683469	23.857703
129.247947	3874.796199	23.862720
129.085699	3897.792428	23.867738
129.559693	3890.188818	23.872755
129.432130	3881.454778	23.877773
129.587094	3881.954761	23.882791
129.671321	3906.335500	23.887808
129.926612	3903.042090	23.892826
129.983633	3906.172448	23.897843
130.240084	3904.796657	23.902861
129.926763	3932.524223	23.907879
130.537119	3898.384696	23.912896
130.307206	3919.779945	23.917914
130.664788	3909.722508	23.922931
130.746279	3908.849738	23.927949
130.769432	3920.422896	23.932967
131.167124	3936.565667	23.937984
131.206105	3927.831002	23.943002
131.268739	3917.557854	23.948019
131.535151	3951.317723	23.953037
131.067897	3919.507706	23.958055
131.129078	3928.585121	23.963072
131.298129	3933.466755	23.968090
131.666875	3948.146301	23.973107
131.710796	3945.401829	23.978125
131.738394	3971.063690	23.983143
132.231853	3957.256699	23.988160
132.071829	3956.054293	23.993178
132.272987	3989.464376	23.998195
132.921572	3978.265497	24.003213
132.687419	3986.479904	24.008231
132.632810	3993.377179	24.013248
132.803382	3975.133121	24.018266
132.673031	3980.417282	24.023283
132.941573	4003.606150	24.028301
133.319219	3998.682968	24.033319
133.378312	3996.226335	24.038336
133.153340	4018.702564	24.043354
133.371458	4017.843401	24.048371
133.766381	4018.595396	24.053389
133.833857	4032.836137	24.058407
134.048800	4031.890164	24.063424
133.966190	4032.213282	24.068442
134.204283	4040.290274	24.073459
134.215256	4064.192882	24.078477
134.373305	4061.252411	24.083495
134.885098	4057.655330	24.088512
134.496299	4078.453914	24.093530
134.895762	4082.131487	24.098547
135.038339	4091.609797	24.103565
135.322103	4096.640749	24.108583
135.460967	4083.569838	24.113600
135.552107	4099.933945	24.118618
135.833292	4090.498999	24.123635
135.917802	4089.959273	24.128653
136.076315	4098.568169	24.133671
136.550453	4096.909859	24.138688
136.321490	4109.500373	24.143706
136.794889	4111.413528	24.148723
136.534227	4103.432154	24.153741
136.406225	4114.953262	24.158759
136.973888	4107.567452	24.163776
136.718242	4115.260668	24.168794
137.006058	4111.710302	24.173811
137.309757	4124.519539	24.178829
137.148000	4134.506588	24.183847
137.546961	4125.482347	24.188864
137.508642	4146.895363	24.193882
137.856576	4123.310642	24.198899
137.529712	4137.229695	24.203917
137.810259	4155.719850	24.208935
138.138794	4159.078362	24.213952
138.142158	4147.960995	24.218970
138.275014	4152.571576	24.223987
138.620273	4177.143206	24.229005
138.486653	4149.396787	24.234023
138.863641	4179.796320	24.239040
139.065716	4199.584420	24.244058
139.013855	4187.613666	24.249075
139.100652	4175.034762	24.254093
138.840640	4195.462133	24.259111
139.318854	4186.419712	24.264128
139.541509	4186.052257	24.269146
139.516618	4184.669382	24.274163
139.725979	4206.895716	24.279181
139.908074	4211.631408	24.284199
140.301719	4200.874200	24.289216
140.201746	4206.673572	24.294234
139.881031	4214.943600	24.299251
140.455499	4214.420931	24.304269
140.249849	4257.831840	24.309287
140.616243	4222.212230	24.314304
140.878257	4208.766008	24.319322
140.713028	4248.509394	24.324339
140.705804	4284.060020	24.329357
140.620443	4256.692736	24.334375
141.270575	4255.464177	24.339392
141.389333	4318.192412	24.344410
141.553318	4284.219137	24.349427
141.824563	4299.666621	24.354445
141.886617	4285.379030	24.359463
142.591044	4302.349627	24.364480
142.132411	4326.016812	24.369498
142.407434	4318.591027	24.374515
142.409245	4331.877308	24.379533
142.714712	4301.600727	24.384551
142.603046	4344.713712	24.389568
142.546035	4333.193626	24.394586
142.938622	4332.626796	24.399603
142.997552	4369.625536	24.404621
143.306635	4355.923878	24.409639
143.316132	4373.489942	24.414656
143.425717	4363.140558	24.419674
143.895393	4364.609096	24.424691
144.095451	4370.315854	24.429709
143.883296	4407.648189	24.434727
144.477334	4376.278403	24.439744
144.676550	4404.087973	24.444762
144.638867	4412.283876	24.449779
144.708776	4387.321575	24.454797
144.474481	4404.294863	24.459815
145.289929	4423.360860	24.464832
145.233580	4415.736132	24.469850
144.972200	4436.992406	24.474867
145.427641	4407.358781	24.479885
145.139002	4451.540258	24.484903
145.757531	4446.776759	24.489920
145.744375	4464.363850	24.494938
145.984230	4463.680556	24.499955
146.407588	4444.683683	24.504973
146.056417	4464.772752	24.509991
146.420669	4436.098388	24.515008
146.181764	4473.527981	24.520026
146.740297	4467.791503	24.525043
146.859126	4478.968317	24.530061
146.568086	4476.553272	24.535079
147.093462	4465.927481	24.540096
147.412433	4486.262939	24.545114
147.089180	4492.226249	24.550131
147.447546	4521.477003	24.555149
147.418530	4499.389804	24.560167
147.523595	4520.396611	24.565184
147.819466	4512.026557	24.570202
148.012205	4522.707035	24.575219
148.239517	4528.782388	24.580237
148.116857	4533.417310	24.585255
148.498109	4540.250853	24.590272
148.617367	4528.726895	24.595290
148.284504	4566.398263	24.600307
148.840462	4536.398287	24.605325
148.653427	4577.315020	24.610343
149.179759	4564.026930	24.615360
149.134287	4610.976148	24.620378
149.084318	4580.205001	24.625395
149.945312	4569.511464	24.630413
149.794157	4639.371965	24.635431
149.761227	4630.563388	24.640448
149.962545	4592.720118	24.645466
149.910888	4628.212581	24.650483
150.496106	4597.994627	24.655501
150.329862	4651.511449	24.660519
150.682532	4620.801098	24.665536
150.684465	4643.704662	24.670554
150.878204	4628.371498	24.675571
151.249668	4674.550373	24.680589
151.071513	4645.650563	24.685607
151.340557	4669.364328	24.690624
151.338106	4654.805822	24.695642
151.629874	4688.195185	24.700659
152.140787	4683.586439	24.705677
152.019117	4696.517495	24.710695
152.200146	4696.770270	24.715712
152.252658	4703.071808	24.720730
152.537485	4713.902944	24.725747
152.800417	4715.028456	24.730765
152.910613	4718.467539	24.735783
152.742208	4732.372900	24.740800
153.098013	4700.597513	24.745818
153.256467	4736.281725	24.750835
153.547199	4719.791536	24.755853
153.679790	4753.008972	24.760871
153.903508	4721.664458	24.765888
154.152965	4743.211820	24.770906
154.017885	4742.152477	24.775923
154.612548	4729.506285	24.780941
154.444913	4756.944705	24.785959
154.752804	4747.539697	24.790976
154.810780	4774.968926	24.795994
154.631259	4762.833187	24.801011
155.004429	4775.814430	24.806029
154.730444	4765.908244	24.811047
154.888025	4777.190815	24.816064
155.157134	4765.289561	24.821082
154.871573	4801.101366	24.826099
155.614619	4791.523893	24.831117
155.442648	4793.676139	24.836135
155.586965	4837.309082	24.841152
156.413188	4810.754383	24.846170
155.901403	4831.568916	24.851187
156.418909	4834.149325	24.856205
156.244339	4823.084992	24.861223
156.620673	4858.233647	24.866240
157.008794	4844.895755	24.871258
156.538682	4869.952557	24.876275
156.739952	4859.150812	24.881293
157.080685	4886.983574	24.886311
157.127500	4872.515332	24.891328
157.426090	4867.410947	24.896346
157.241696	4916.560037	24.901363
157.751895	4900.815045	24.906381
157.769251	4915.055194	24.911399
158.482081	4942.707586	24.916416
158.282396	4924.357756	24.921434
158.557909	4946.872031	24.926451
159.090679	4922.664976	24.931469
159.030167	4955.643825	24.936487
159.165413	4924.810958	24.941504
159.075871	4945.414365	24.946522
159.435335	4975.506817	24.951539
159.438721	4965.579873	24.956557
159.626931	4948.842235	24.961575
159.513007	4989.233963	24.966592
159.925027	4977.681070	24.971610
159.839465	5003.279388	24.976627
159.873914	5008.774434	24.981645
160.140210	5019.528509	24.986663
160.499911	5038.240806	24.991680
160.435640	5015.651037	24.996698
160.575721	5062.037161	25.001715
161.098034	5035.307882	25.006733
161.447674	5086.420935	25.011751
161.457673	5054.222400	25.016768
161.780637	5062.437473	25.021786
161.723708	5061.804620	25.026803
162.113290	5086.710561	25.031821
162.289684	5049.897511	25.036839
162.264563	5092.965849	25.041856
162.161450	5060.612262	25.046874
162.557547	5092.801154	25.051891
162.636215	5082.760645	25.056909
162.792576	5116.735844	25.061927
163.084968	5091.635392	25.066944
162.989358	5105.501177	25.071962
163.230137	5087.537984	25.076979
163.551000	5102.618888	25.081997
163.582784	5118.280063	25.087015
163.529361	5119.685761	25.092032
163.811219	5111.774674	25.097050
163.736987	5127.555031	25.102067
164.419031	5144.317775	25.107085
164.195651	5138.573546	25.112103
164.441887	5152.779793	25.117120
164.528993	5160.586469	25.122138
164.671809	5167.304131	25.127155
164.747170	5174.526598	25.132173
165.086710	5195.623645	25.137191
165.106216	5172.299662	25.142208
165.104623	5216.477787	25.147226
165.501931	5200.285537	25.152243
165.281325	5219.744336	25.157261
166.026080	5223.596081	25.162279
165.945793	5247.324782	25.167296
166.574261	5246.031952	25.172314
166.288883	5244.773112	25.177331
166.715130	5260.707467	25.182349
166.840706	5271.493605	25.187367
166.789884	5273.858681	25.192384
167.536604	5249.015153	25.197402
167.077342	5291.885025	25.202419
167.680486	5265.254156	25.207437
166.966216	5319.556224	25.212455
167.189460	5296.314421	25.217472
168.200757	5316.614600	25.222490
167.876571	5332.489311	25.227507
168.153976	5339.915658	25.232525
168.716991	5337.334404	25.237543
168.666724	5346.208614	25.242560
169.145612	5343.663587	25.247578
169.004088	5353.569563	25.252595
169.351359	5349.491772	25.257613
169.556503	5332.850124	25.262631
169.347920	5353.686278	25.267648
170.149636	5338.662958	25.272666
169.639767	5388.352485	25.277683
170.112599	5355.777402	25.282701
170.448052	5384.314480	25.287719
170.369610	5361.131688	25.292736
170.496250	5371.536963	25.297754
170.703970	5397.558084	25.302771
170.747331	5376.075597	25.307789
170.782681	5414.518828	25.312807
170.943761	5394.799444	25.317824
171.820426	5431.653173	25.322842
171.441483	5412.847484	25.327859
171.331378	5436.412887	25.332877
171.562305	5429.723647	25.337895
171.983598	5406.628678	25.342912
172.182855	5443.024793	25.347930
172.018236	5462.185474	25.352947
171.922707	5448.961126	25.357965
172.779206	5439.183424	25.362983
172.809099	5504.276863	25.368000
173.150393	5479.862625	25.373018
172.835335	5507.622536	25.378035
172.678550	5497.757746	25.383053
173.474060	5489.718148	25.388071
173.202831	5495.181080	25.393088
173.625638	5500.435022	25.398106
173.812955	5525.516351	25.403123
174.292327	5512.463837	25.408141
174.126424	5542.144794	25.413159
174.389736	5518.253506	25.418176
174.486466	5571.532701	25.423194
174.317391	5548.427789	25.428211
174.716892	5563.265334	25.433229
175.196215	5582.150427	25.438247
175.014466	5574.569478	25.443264
175.465945	5601.334882	25.448282
175.684809	5592.102452	25.453299
176.068017	5610.801505	25.458317
176.011191	5619.806734	25.463335
176.320729	5615.336020	25.468352
176.314087	5623.052468	25.473370
176.883772	5620.223074	25.478387
176.890783	5670.975036	25.483405
176.994344	5668.567681	25.488423
177.039371	5638.436090	25.493440
177.384755	5644.603225	25.498458
177.344211	5652.220459	25.503475
177.803195	5652.923003	25.508493
177.950481	5657.790591	25.513511
177.731691	5673.241340	25.518528
178.276491	5684.842861	25.523546
178.404130	5690.069979	25.528563
178.604941	5702.071729	25.533581
178.793807	5703.987202	25.538599
178.751568	5694.565826	25.543616
178.999111	5731.343597	25.548634
178.600968	5730.566073	25.553651
179.367015	5719.431345	25.558669
179.318249	5765.240079	25.563687
179.364719	5743.951670	25.568704
179.872180	5759.444067	25.573722
180.058576	5768.781159	25.578739
180.227118	5775.760126	25.583757
180.164661	5778.589735	25.588775
180.235553	5764.413377	25.593792
180.656693	5807.765895	25.598810
180.727160	5789.332577	25.603827
181.361816	5832.692825	25.608845
181.936991	5815.451942	25.613863
181.777244	5813.734024	25.618880
182.174734	5841.458058	25.623898
182.049893	5815.037462	25.628915
182.074327	5840.617335	25.633933
182.338996	5820.822650	25.638951
182.181986	5816.182372	25.643968
182.300014	5826.175521	25.648986
182.584983	5849.149124	25.654003
183.118831	5854.092826	25.659021
183.283336	5835.332125	25.664039
183.013095	5857.648436	25.669056
183.508289	5866.016666	25.674074
183.547419	5860.752691	25.679092
183.793820	5882.119690	25.684109
184.063719	5886.266825	25.689127
184.372656	5885.186958	25.694144
184.426221	5902.168783	25.699162
184.565998	5901.270085	25.704180
184.376869	5929.360807	25.709197
184.500496	5900.235764	25.714215
184.559740	5934.349490	25.719232
184.718175	5945.621808	25.724250
185.421932	5946.814033	25.729268
185.493231	5961.437602	25.734285
185.510704	5966.928632	25.739303
186.053299	5983.147333	25.744320
186.560231	5968.846190	25.749338
186.370154	6010.623355	25.754356
186.377925	5998.953169	25.759373
186.678413	5995.977021	25.764391
186.477484	6037.039270	25.769408
186.954593	6026.261145	25.774426
187.258978	6051.696048	25.779444
187.141610	6040.904905	25.784461
187.276488	6067.040312	25.789479
187.456851	6068.378932	25.794496
187.555639	6087.922484	25.799514
188.215166	6065.466684	25.804532
188.368342	6114.126152	25.809549
188.569126	6100.458245	25.814567
188.719060	6093.980667	25.819584
188.913021	6140.895797	25.824602
188.977127	6137.008488	25.829620
189.195570	6155.408789	25.834637
189.489839	6138.581303	25.839655
189.363986	6167.604128	25.844672
190.125630	6162.011648	25.849690
190.021922	6143.999819	25.854708
190.160307	6185.662959	25.859725
190.943131	6162.692489	25.864743
190.593517	6204.756051	25.869760
191.012846	6158.991538	25.874778
190.960367	6203.069796	25.879796
190.951964	6193.846475	25.884813
191.324309	6225.398858	25.889831
191.813664	6204.670154	25.894848
191.987564	6212.134688	25.899866
191.995805	6220.586263	25.904884
192.031667	6221.503418	25.909901
192.531544	6246.113657	25.914919
192.503209	6230.323302	25.919936
192.445690	6269.781957	25.924954
192.605026	6238.036953	25.929972
192.741001	6282.128673	25.934989
193.117416	6262.178689	25.940007
193.170448	6308.163270	25.945024
193.370566	6284.484592	25.950042
193.403937	6319.814152	25.955060
193.857121	6301.204315	25.960077
193.870459	6348.504514	25.965095
194.091368	6338.670997	25.970112
194.465329	6327.346566	25.975130
194.931623	6373.441700	25.980148
194.602651	6368.281863	25.985165
195.409443	6343.352980	25.990183
195.517446	6372.231924	25.995200
195.539947	6393.393823	26.000218
195.495534	6370.099381	26.005236
195.848154	6365.378468	26.010253
196.224658	6415.164583	26.015271
196.202778	6420.231695	26.020288
196.513733	6385.498462	26.025306
196.587293	6424.895722	26.030324
196.587526	6462.639978	26.035341
196.888032	6449.867714	26.040359
197.000138	6433.312833	26.045376
197.505173	6442.784444	26.050394
197.728414	6500.512502	26.055412
197.650429	6474.155639	26.060429
198.714825	6485.455454	26.065447
198.376405	6497.046582	26.070464
198.638398	6464.195053	26.075482
199.071048	6497.559768	26.080500
198.756483	6499.968660	26.085517
199.474300	6468.944497	26.090535
199.563862	6480.421749	26.095552
199.628245	6531.274518	26.100570
199.752054	6528.857503	26.105588
199.529433	6520.642938	26.110605
200.341182	6513.988073	26.115623
200.424994	6579.526897	26.120640
200.376160	6571.506468	26.125658
200.719014	6546.060343	26.130676
200.951535	6540.711009	26.135693
200.840234	6581.987856	26.140711
200.892841	6617.593577	26.145728
201.224520	6632.368273	26.150746
201.467595	6636.767733	26.155764
200.954680	6617.357947	26.160781
202.094334	6602.919923	26.165799
202.234050	6610.721341	26.170816
202.326859	6661.405589	26.175834
202.248827	6649.823313	26.180852
202.644572	6641.071865	26.185869
202.824346	6683.780156	26.190887
202.766866	6676.602114	26.195904
202.988850	6683.547030	26.200922
203.254111	6683.751801	26.205940
204.057242	6684.062011	26.210957
204.646880	6685.504599	26.215975
205.234304	6727.077222	26.220992
204.721052	6706.929371	26.226010
205.482845	6674.284086	26.231028
205.600107	6689.148884	26.236045
205.752488	6708.409341	26.241063
205.493248	6696.830739	26.246080
205.705095	6687.273809	26.251098
206.055455	6667.635065	26.256116
205.772580	6713.928588	26.261133
206.197150	6701.966382	26.266151
205.992020	6699.101387	26.271168
206.130993	6709.260953	26.276186
206.644300	6682.966810	26.281204
206.552999	6717.223573	26.286221
206.685516	6762.906574	26.291239
206.668969	6789.307368	26.296256
206.770684	6787.282505	26.301274
207.178840	6775.680843	26.306292
207.373367	6824.239282	26.311309
207.585964	6801.294221	26.316327
207.811499	6832.288299	26.321344
207.998075	6863.478268	26.326362
208.524545	6846.668827	26.331380
208.967233	6862.424489	26.336397
209.110570	6896.620656	26.341415
209.125683	6876.278191	26.346432
208.986558	6916.805088	26.351450
209.498845	6903.104880	26.356468
209.964340	6884.309818	26.361485
210.295874	6909.146274	26.366503
210.707404	6958.638310	26.371520
210.494761	6961.016863	26.376538
210.717837	6962.650886	26.381556
210.745403	6967.566319	26.386573
211.100688	6945.388230	26.391591
211.351164	6961.892196	26.396608
211.504036	6990.225453	26.401626
212.244601	6984.901187	26.406644
211.768787	6987.656872	26.411661
212.025393	7005.906593	26.416679
212.398879	7023.571997	26.421696
212.623475	7011.875889	26.426714
212.479782	7033.578974	26.431732
212.985634	7039.455182	26.436749
213.205923	7056.351170	26.441767
213.760225	7036.626713	26.446784
213.778570	7042.030668	26.451802
213.909094	7080.939859	26.456820
213.978847	7104.061452	26.461837
214.217470	7098.083867	26.466855
214.660033	7062.578251	26.471872
214.458123	7113.649352	26.476890
214.718921	7099.815961	26.481908
214.795155	7091.054603	26.486925
214.968630	7118.823046	26.491943
215.240565	7159.209542	26.496960
215.304782	7178.462634	26.501978
216.084083	7170.866133	26.506996
216.207763	7150.281746	26.512013
216.381469	7160.541516	26.517031
216.494294	7207.886823	26.522048
216.624796	7194.126044	26.527066
216.825642	7200.039925	26.532084
216.738053	7229.888807	26.537101
216.716335	7227.352467	26.542119
217.673785	7226.872534	26.547136
217.430274	7280.906089	26.552154
217.966552	7260.325801	26.557172
218.341339	7272.368762	26.562189
218.127995	7288.048495	26.567207
218.700404	7264.211343	26.572224
218.876739	7315.848354	26.577242
219.059375	7317.487291	26.582260
218.938642	7311.747088	26.587277
219.709287	7312.395322	26.592295
220.071934	7358.776780	26.597312
220.068625	7362.668901	26.602330
220.689490	7351.232736	26.607348
221.125289	7324.781440	26.612365
220.711001	7369.107317	26.617383
220.928830	7343.169119	26.622400
221.230687	7379.919518	26.627418
221.553687	7404.247522	26.632436
221.569809	7392.183860	26.637453
222.100793	7379.649445	26.642471
222.359490	7377.601051	26.647488
222.265597	7420.675326	26.652506
222.444680	7441.189027	26.657524
222.950598	7448.251912	26.662541
222.814531	7441.223721	26.667559
223.317451	7423.409472	26.672576
223.312866	7458.654953	26.677594
223.649971	7448.137320	26.682612
223.381461	7490.999655	26.687629
223.664418	7462.005871	26.692647
224.032767	7507.120893	26.697664
224.240956	7508.055507	26.702682
224.424532	7511.958789	26.707700
224.737678	7548.779407	26.712717
225.143437	7543.347022	26.717735
225.293038	7559.503436	26.722752
225.428880	7554.827726	26.727770
225.494142	7576.183563	26.732788
225.863012	7559.225344	26.737805
225.827008	7608.976585	26.742823
226.537488	7574.582104	26.747840
225.931699	7629.538610	26.752858
226.376370	7603.157008	26.757876
226.667666	7665.735051	26.762893
226.322210	7671.941571	26.767911
227.263261	7655.964481	26.772928
227.317097	7713.023199	26.777946
227.708500	7685.221843	26.782964
227.786810	7732.169104	26.787981
228.004185	7710.613791	26.792999
228.595352	7740.554565	26.798016
228.469640	7748.475219	26.803034
229.159758	7760.889268	26.808052
229.313973	7760.255685	26.813069
229.304788	7801.245820	26.818087
229.860148	7780.021292	26.823104
230.228617	7796.788280	26.828122
230.363252	7801.303732	26.833140
230.592499	7798.544742	26.838157
230.548069	7810.801321	26.843175
231.267772	7815.184957	26.848192
231.203450	7826.933276	26.853210
231.254657	7842.620204	26.858228
231.791120	7853.719625	26.863245
232.065922	7857.946799	26.868263
232.152449	7869.157298	26.873280
232.470914	7883.238999	26.878298
232.676275	7892.156993	26.883316
232.647249	7897.010940	26.888333
232.891405	7901.089577	26.893351
233.133899	7906.462050	26.898368
233.239147	7924.860566	26.903386
233.696797	7938.920919	26.908404
233.988525	7955.513838	26.913421
233.915325	7962.323077	26.918439
234.007053	7981.591709	26.923456
234.484087	7994.482918	26.928474
234.875375	8004.893499	26.933492
235.142978	8007.780288	26.938509
234.899192	8009.471541	26.943527
235.673325	8041.759253	26.948544
235.507838	8029.020582	26.953562
235.826767	8073.061708	26.958580
236.110986	8052.000406	26.963597
236.198532	8091.095346	26.968615
236.971280	8077.680667	26.973632
236.867342	8108.991954	26.978650
237.303270	8104.494063	26.983668
237.508178	8128.822410	26.988685
237.671114	8138.281983	26.993703
238.113882	8128.329303	26.998720
237.731580	8124.112915	27.003738
237.900637	8139.010251	27.008756
238.272581	8160.355808	27.013773
238.215981	8166.529862	27.018791
238.436939	8177.576743	27.023808
239.092051	8186.717899	27.028826
239.205360	8218.655746	27.033844
239.517699	8190.554458	27.038861
239.504626	8250.924412	27.043879
240.103277	8227.925847	27.048896
240.277602	8258.141845	27.053914
240.341682	8262.913399	27.058932
240.871946	8257.715856	27.063949
241.027288	8309.339204	27.068967
241.435231	8290.867872	27.073984
241.494484	8304.179250	27.079002
241.982337	8321.563588	27.084020
242.517347	8333.706986	27.089037
241.915668	8327.156257	27.094055
242.445513	8358.158519	27.099072
242.568481	8358.304170	27.104090
242.711458	8369.816861	27.109108
243.265700	8369.988976	27.114125
243.491352	8400.909984	27.119143
244.081206	8399.849694	27.124160
243.605041	8437.287765	27.129178
244.285285	8425.555689	27.134196
244.486028	8446.405679	27.139213
244.378202	8449.271352	27.144231
244.916390	8473.778476	27.149248
245.218738	8482.904445	27.154266
246.309533	8443.775680	27.159284
247.626988	8440.090861	27.164301
247.843543	8416.148081	27.169319
247.744102	8441.860772	27.174336
248.242086	8413.279383	27.179354
247.723204	8407.525107	27.184372
248.153840	8396.386799	27.189389
247.940071	8381.987359	27.194407
247.898193	8380.561159	27.199424
248.115566	8388.482544	27.204442
247.976117	8390.214648	27.209460
248.328340	8407.155669	27.214477
248.393319	8413.024024	27.219495
248.735719	8425.232824	27.224512
248.930820	8453.414209	27.229530
248.739542	8452.752263	27.234548
249.242437	8474.363034	27.239565
249.141162	8485.687343	27.244583
249.402358	8500.779663	27.249600
249.622097	8521.060181	27.254618
249.945000	8561.588723	27.259636
250.412988	8557.625388	27.264653
250.340118	8585.989803	27.269671
250.628491	8596.691040	27.274688
250.791199	8586.905455	27.279706
250.874454	8626.390415	27.284724
251.946108	8622.464607	27.289741
251.800327	8650.949357	27.294759
252.227704	8649.674166	27.299776
252.496359	8657.152374	27.304794
252.354193	8662.994831	27.309812
252.735675	8680.988283	27.314829
253.002993	8700.303823	27.319847
253.154326	8702.853612	27.324864
253.335191	8746.485952	27.329882
253.633088	8742.767650	27.334900
253.971123	8768.969073	27.339917
253.887397	8786.805462	27.344935
254.733984	8795.323164	27.349952
254.853031	8806.329709	27.354970
254.666202	8818.531519	27.359988
255.092477	8831.202565	27.365005
255.393871	8856.524729	27.370023
255.725016	8868.649916	27.375040
256.258341	8884.659259	27.380058
256.536008	8899.340960	27.385076
257.057094	8910.603764	27.390093
257.145063	8918.429598	27.395111
257.385132	8934.904369	27.400128
257.757074	8950.210447	27.405146
257.473878	8949.014661	27.410164
257.906155	8977.129721	27.415181
257.981130	8988.705272	27.420199
258.795836	8994.069162	27.425216
258.587828	9015.054349	27.430234
259.024320	9034.335487	27.435252
259.335421	9046.191353	27.440269
259.642768	9057.604012	27.445287
259.896324	9063.460663	27.450304
260.203947	9072.004239	27.455322
260.415363	9100.021355	27.460340
261.000111	9099.457589	27.465357
260.966023	9114.423693	27.470375
261.460456	9118.274705	27.475392
261.464049	9105.578588	27.480410
261.452515	9151.361917	27.485428
262.119534	9142.642109	27.490445
262.154561	9165.700436	27.495463
262.278375	9162.138833	27.500480
262.482426	9201.320409	27.505498
262.926342	9208.147332	27.510516
262.898590	9207.382954	27.515533
263.131748	9253.964867	27.520551
263.679053	9248.840211	27.525568
264.042905	9276.433608	27.530586
263.730349	9298.856238	27.535604
264.288712	9306.410961	27.540621
264.351659	9316.597020	27.545639
264.763726	9334.903516	27.550656
265.090942	9357.925007	27.555674
265.692762	9379.351350	27.560692
266.026171	9373.372707	27.565709
265.798761	9385.725058	27.570727
266.410197	9386.455056	27.575744
266.602228	9416.881080	27.580762
266.886670	9410.297215	27.585780
267.378499	9420.580237	27.590797
267.433558	9459.888539	27.595815
267.681226	9450.165181	27.600832
268.098275	9457.260515	27.605850
268.077747	9495.826692	27.610868
268.357487	9489.013367	27.615885
268.513251	9505.723725	27.620903
268.712856	9519.774381	27.625920
268.946485	9536.229595	27.630938
269.127116	9559.410507	27.635956
269.921943	9544.724844	27.640973
269.683738	9579.554576	27.645991
269.770735	9615.845430	27.651008
270.492793	9590.018520	27.656026
270.651097	9639.673548	27.661044
271.080369	9625.813335	27.666061
271.078217	9675.776567	27.671079
271.865893	9671.944166	27.676096
271.841938	9687.496281	27.681114
271.962649	9715.630522	27.686132
272.218412	9718.179973	27.691149
272.687571	9719.923425	27.696167
273.046610	9738.907373	27.701184
273.503463	9758.073670	27.706202
273.916519	9755.307457	27.711220
274.072636	9780.078697	27.716237
274.256528	9804.461522	27.721255
274.612715	9799.567423	27.726272
275.088218	9813.785279	27.731290
275.007806	9820.450927	27.736308
275.394390	9818.557315	27.741325
275.328598	9858.256574	27.746343
275.401835	9871.255488	27.751360
275.965593	9878.073064	27.756378
276.091541	9906.861962	27.761396
276.213963	9896.845862	27.766413
276.745234	9927.138581	27.771431
276.946862	9950.408038	27.776448
277.610622	9939.389614	27.781466
277.534644	9974.898330	27.786484
278.360330	9969.947443	27.791501
278.241199	9988.674257	27.796519
278.467477	10015.068415	27.801536
278.800722	10017.973076	27.806554
279.225692	10013.124213	27.811572
279.334628	10067.695183	27.816589
279.491412	10043.636964	27.821607
279.873393	10059.776361	27.826624
280.097818	10087.757446	27.831642
280.540719	10096.217093	27.836660
280.695831	10080.827426	27.841677
281.024995	10119.356387	27.846695
281.358409	10099.939742	27.851712
281.205581	10139.057494	27.856730
282.017119	10122.466135	27.861748
282.150120	10141.806129	27.866765
282.276972	10186.407431	27.871783
282.173200	10159.780594	27.876800
282.566546	10201.637433	27.881818
282.796173	10202.121814	27.886836
282.916409	10238.351035	27.891853
283.375207	10247.267821	27.896871
283.618458	10272.489115	27.901888
283.846983	10305.307441	27.906906
284.032294	10314.071509	27.911924
284.575519	10320.170911	27.916941
284.719172	10369.979820	27.921959
284.995261	10357.715331	27.926976
285.624751	10383.967567	27.931994
285.696195	10399.693300	27.937012
285.931534	10419.740569	27.942029
286.383565	10446.284836	27.947047
286.859640	10458.478720	27.952064
287.394097	10464.389131	27.957082
287.376440	10474.077289	27.962100
287.699325	10492.713817	27.967117
288.034724	10507.108914	27.972135
288.271452	10528.737149	27.977152
288.822226	10519.746658	27.982170
288.799029	10520.655787	27.987188
289.240344	10563.453514	27.992205
289.475861	10564.843180	27.997223
289.536342	10606.995413	28.002240
290.519030	10598.538078	28.007258
290.205315	10631.208233	28.012276
290.980139	10600.420656	28.017293
290.772698	10649.908306	28.022311
291.212035	10631.935923	28.027328
291.776996	10660.340713	28.032346
292.008120	10688.016891	28.037364
291.889982	10685.597246	28.042381
292.213682	10696.884998	28.047399
292.116424	10729.059294	28.052416
292.797199	10707.097253	28.057434
292.952418	10778.647466	28.062452
293.207979	10758.263364	28.067469
293.498669	10804.854301	28.072487
293.667377	10793.415211	28.077504
294.010352	10852.776791	28.082522
294.437230	10870.868744	28.087540
294.718956	10853.774720	28.092557
295.080819	10883.294817	28.097575
295.072686	10907.988244	28.102592
295.831912	10927.860220	28.107610
296.163676	10920.812092	28.112628
296.505928	10956.748339	28.117645
296.662505	10939.166942	28.122663
296.742805	10980.733893	28.127680
297.078238	10976.716695	28.132698
297.656476	10972.779244	28.137716
297.331873	11032.960960	28.142733
297.923079	11016.735469	28.147751
298.303970	11032.159520	28.152768
298.572368	11059.801716	28.157786
298.951719	11086.148961	28.162804
299.094606	11096.671740	28.167821
299.404768	11103.967879	28.172839
299.233671	11136.395244	28.177856
299.902237	11121.950126	28.182874
299.939954	11175.298100	28.187892
300.068141	11165.166909	28.192909
300.941694	11200.755607	28.197927
301.352844	11218.183097	28.202944
301.967557	11217.886020	28.207962
301.499152	11254.297287	28.212980
302.137629	11240.073283	28.217997
302.395614	11283.507102	28.223015
302.785420	11281.764698	28.228032
303.238455	11313.014750	28.233050
303.723438	11322.847643	28.238068
303.558931	11347.735529	28.243085
304.539478	11336.552280	28.248103
304.549263	11388.067365	28.253120
304.994964	11378.923120	28.258138
304.830443	11408.735917	28.263156
305.536919	11393.318426	28.268173
306.008867	11430.275188	28.273191
306.010432	11424.328563	28.278208
306.381640	11452.007036	28.283226
306.766760	11477.008621	28.288244
306.895160	11471.469907	28.293261
307.513346	11496.617364	28.298279
307.650270	11521.097819	28.303296
307.966561	11508.099955	28.308314
307.824669	11541.647416	28.313332
308.458259	11541.010477	28.318349
308.702351	11573.621704	28.323367
308.959668	11564.115822	28.328384
309.343166	11598.947935	28.333402
309.917552	11604.610033	28.338420
309.790276	11602.517135	28.343437
310.285269	11646.286886	28.348455
310.893135	11630.670011	28.353472
311.335957	11674.986101	28.358490
311.015340	11673.881049	28.363508
311.861906	11679.328222	28.368525
312.072313	11696.748123	28.373543
312.338000	11716.278346	28.378560
312.647800	11708.225548	28.383578
312.746581	11685.010584	28.388596
312.880116	11748.982569	28.393613
313.141534	11746.769855	28.398631
313.405912	11759.699405	28.403648
313.814590	11772.347817	28.408666
314.039298	11784.051590	28.413684
313.953250	11801.673515	28.418701
314.550983	11827.196664	28.423719
314.611070	11840.529936	28.428736
314.878909	11885.023283	28.433754
315.321668	11892.655603	28.438772
315.145395	11910.815817	28.443789
315.720256	11924.386663	28.448807
315.616014	11963.440794	28.453824
316.389571	11975.281160	28.458842
316.844579	12010.980394	28.463860
317.280613	12045.988156	28.468877
318.065301	12029.938144	28.473895
318.278014	12067.187476	28.478912
318.452984	12083.111562	28.483930
318.808762	12087.611172	28.488948
319.363411	12103.615456	28.493965
319.717403	12126.771909	28.498983
319.905210	12125.702868	28.504000
320.414797	12148.649990	28.509018
320.512370	12176.345266	28.514036
320.899044	12168.390951	28.519053
320.947729	12192.870816	28.524071
321.462058	12218.456326	28.529088
321.759797	12223.803258	28.534106
322.019912	12250.581803	28.539124
321.959656	12275.736762	28.544141
322.650574	12264.404990	28.549159
323.062674	12314.851662	28.554176
323.260095	12309.037777	28.559194
323.273224	12332.187673	28.564212
323.363893	12383.842801	28.569229
324.605939	12388.885227	28.574247
324.371893	12414.819379	28.579264
324.629574	12433.026167	28.584282
325.314070	12448.621504	28.589300
325.426376	12461.361018	28.594317
325.528090	12493.830650	28.599335
326.323391	12502.262459	28.604352
326.852314	12515.582999	28.609370
327.038029	12560.638444	28.614388
327.299985	12560.107139	28.619405
327.776402	12553.614897	28.624423
327.804300	12602.235930	28.629440
328.022187	12587.508247	28.634458
328.507518	12633.763694	28.639476
329.162398	12602.249550	28.644493
329.747475	12651.965530	28.649511
329.657480	12641.202642	28.654528
330.102470	12670.072101	28.659546
330.404443	12644.498021	28.664564
330.405120	12695.104404	28.669581
331.040049	12668.069505	28.674599
331.337953	12728.410417	28.679616
331.220506	12691.762953	28.684634
331.784796	12734.955549	28.689652
332.265374	12720.956833	28.694669
332.771561	12747.907000	28.699687
333.154954	12786.692894	28.704704
333.153802	12759.096271	28.709722
333.350237	12818.598926	28.714740
333.672981	12808.186517	28.719757
333.909232	12823.312353	28.724775
333.997910	12842.418478	28.729792
334.285566	12870.449157	28.734810
334.486411	12892.599495	28.739828
335.003378	12911.818683	28.744845
335.541248	12925.134028	28.749863
335.688673	12964.428475	28.754880
336.024742	12989.046434	28.759898
336.669196	13001.606159	28.764916
336.787129	13029.147049	28.769933
337.301932	13035.709808	28.774951
337.433329	13060.029717	28.779968
337.990069	13099.983623	28.784986
338.801525	13092.643956	28.790004
338.580020	13109.355467	28.795021
338.914678	13134.897174	28.800039
339.199037	13165.488429	28.805056
339.381588	13174.879576	28.810074
339.862801	13186.954632	28.815092
339.881441	13228.753055	28.820109
340.718837	13238.569221	28.825127
340.981274	13269.253123	28.830144
341.505948	13292.787364	28.835162
341.719212	13296.139204	28.840180
342.278976	13326.632188	28.845197
342.899137	13325.741520	28.850215
342.872403	13354.081568	28.855232
343.015521	13370.469011	28.860250
343.627015	13387.623271	28.865268
343.336623	13393.359522	28.870285
343.939602	13439.369229	28.875303
344.424574	13424.914602	28.880320
344.759474	13490.605532	28.885338
345.188332	13478.969277	28.890356
345.474658	13518.871940	28.895373
346.080494	13522.531027	28.900391
346.471149	13541.788856	28.905408
347.007547	13552.501928	28.910426
347.241172	13580.233970	28.915444
347.349532	13591.622167	28.920461
347.813329	13594.547073	28.925479
348.163326	13601.793213	28.930496
348.696837	13625.481040	28.935514
348.572466	13628.742714	28.940532
348.564047	13636.694790	28.945549
349.005866	13668.018407	28.950567
349.487212	13693.445189	28.955584
349.468977	13707.680088	28.960602
350.097006	13725.596908	28.965620
350.124661	13753.742380	28.970637
350.306016	13789.512144	28.975655
350.657477	13784.735117	28.980672
351.023236	13852.779614	28.985690
351.604684	13850.483920	28.990708
352.037017	13902.331907	28.995725
352.684929	13909.775427	29.000743
352.790922	13923.530638	29.005760
353.039672	13944.316046	29.010778
353.774226	13982.467224	29.015796
353.382624	14004.084062	29.020813
354.580473	13993.093832	29.025831
355.008384	14045.522656	29.030848
355.027611	14058.216846	29.035866
355.499251	14091.021394	29.040884
355.791309	14100.191295	29.045901
356.109957	14113.248421	29.050919
356.666659	14139.889756	29.055936
356.769170	14160.152468	29.060954
357.720189	14169.780523	29.065972
357.860438	14186.859945	29.070989
358.243592	14208.949891	29.076007
358.757872	14220.118799	29.081024
359.057066	14245.482843	29.086042
359.594020	14257.889243	29.091060
359.596645	14268.741609	29.096077
360.318666	14260.902510	29.101095
360.262032	14294.049062	29.106112
360.038830	14334.140736	29.111130
360.989873	14333.951014	29.116148
361.222501	14368.145119	29.121165
361.704994	14378.406376	29.126183
362.365912	14409.171457	29.131200
362.224375	14438.422707	29.136218
362.596991	14448.273685	29.141236
362.858986	14469.884538	29.146253
363.322907	14494.795304	29.151271
363.775310	14526.117034	29.156288
363.907539	14544.314761	29.161306
364.700739	14550.158315	29.166324
364.581593	14584.750012	29.171341
365.109668	14613.099924	29.176359
365.367223	14629.171943	29.181376
365.712862	14652.914631	29.186394
365.829764	14675.930029	29.191412
366.139546	14717.186165	29.196429
366.416438	14739.553983	29.201447
366.999819	14757.750623	29.206464
367.149917	14785.696345	29.211482
367.928813	14805.880371	29.216500
368.252864	14827.979156	29.221517
368.491385	14852.038459	29.226535
368.858238	14870.651140	29.231552
369.223861	14887.447044	29.236570
369.943802	14912.296834	29.241588
370.280515	14943.446268	29.246605
370.835800	14949.014189	29.251623
370.812700	14977.982304	29.256640
371.349745	15002.599442	29.261658
372.054378	15008.933653	29.266676
372.123594	15024.438015	29.271693
373.130502	15044.060657	29.276711
373.314826	15048.386364	29.281728
373.738858	15071.204632	29.286746
374.169613	15074.020657	29.291764
374.424404	15101.674158	29.296781
374.749930	15103.156091	29.301799
374.826391	15123.640028	29.306816
374.920877	15140.131884	29.311834
375.547502	15170.187892	29.316852
375.771679	15201.273913	29.321869
376.285507	15200.963554	29.326887
376.529031	15240.785238	29.331904
376.839557	15249.046894	29.336922
377.177819	15275.424502	29.341940
377.530199	15301.276890	29.346957
377.739901	15319.937106	29.351975
378.340289	15343.129066	29.356992
378.385184	15380.761596	29.362010
379.036524	15393.033894	29.367028
379.546740	15423.989077	29.372045
379.786029	15442.009527	29.377063
380.152289	15465.253348	29.382080
380.439981	15490.943370	29.387098
380.951808	15523.148138	29.392116
381.434870	15558.438720	29.397133
382.054468	15577.098979	29.402151
382.732356	15590.907347	29.407168
382.830042	15611.152182	29.412186
382.920497	15627.623654	29.417204
383.955240	15650.616974	29.422221
384.115335	15679.403512	29.427239
384.482635	15693.727712	29.432256
384.729109	15713.150507	29.437274
385.289131	15721.454930	29.442292
385.101618	15751.599596	29.447309
385.389598	15768.278576	29.452327
385.905909	15787.584368	29.457344
386.225956	15826.870873	29.462362
386.883666	15843.054487	29.467380
386.985266	15873.331636	29.472397
387.653811	15898.881059	29.477415
387.973849	15912.410877	29.482432
388.290400	15934.908449	29.487450
388.889839	15949.795397	29.492468
389.322942	15974.908139	29.497485
389.599350	15989.496071	29.502503
389.978784	16011.235245	29.507520
390.006200	16039.764416	29.512538
390.375738	16048.269027	29.517556
390.693011	16068.452905	29.522573
390.754246	16100.976708	29.527591
391.464998	16128.889568	29.532608
391.991476	16154.923988	29.537626
392.421324	16180.073405	29.542644
392.862249	16200.717499	29.547661
393.117250	16234.251386	29.552679
393.472552	16250.837205	29.557696
393.672753	16288.844785	29.562714
393.918683	16301.754177	29.567732
394.687467	16330.146958	29.572749
394.695798	16363.044944	29.577767
395.710382	16384.813048	29.582784
396.043730	16417.487930	29.587802
396.822055	16431.443534	29.592820
397.274969	16460.952678	29.597837
397.215650	16478.509992	29.602855
397.935889	16497.015006	29.607872
398.139325	16511.719870	29.612890
398.298373	16547.034634	29.617908
398.775079	16574.873706	29.622925
399.237502	16604.714241	29.627943
399.739167	16622.975533	29.632960
399.901399	16642.421095	29.637978
400.243012	16683.459267	29.642996
400.307309	16701.532698	29.648013
400.747267	16734.732732	29.653031
401.740667	16759.210896	29.658048
402.033945	16785.107581	29.663066
402.652779	16806.307336	29.668084
403.334788	16810.357418	29.673101
403.498401	16859.635621	29.678119
404.390720	16851.934515	29.683136
404.248209	16881.372036	29.688154
404.587345	16896.720528	29.693172
405.226989	16924.464988	29.698189
405.416297	16944.635076	29.703207
405.836348	16965.059731	29.708224
406.299398	16997.674829	29.713242
406.823034	17020.744963	29.718260
407.192341	17035.811455	29.723277
407.268256	17054.701273	29.728295
408.145362	17081.139812	29.733312
408.098061	17116.083879	29.738330
408.708414	17115.805162	29.743348
409.283599	17150.403495	29.748365
409.295521	17165.589847	29.753383
410.131342	17189.536581	29.758400
410.358055	17211.970915	29.763418
410.738213	17214.295556	29.768436
410.861364	17259.832633	29.773453
411.185432	17252.614359	29.778471
411.565395	17287.157302	29.783488
411.718831	17322.409583	29.788506
412.378529	17332.101244	29.793524
412.392614	17367.337843	29.798541
412.624979	17386.125390	29.803559
413.645628	17411.200205	29.808576
414.097307	17452.494320	29.813594
414.500028	17468.529258	29.818612
415.111625	17487.283667	29.823629
415.610767	17503.325127	29.828647
415.951511	17544.521622	29.833664
416.154952	17570.313673	29.838682
416.656366	17565.731369	29.843700
417.000389	17638.793379	29.848717
417.298629	17637.585125	29.853735
417.758246	17669.330007	29.858752
418.301256	17704.860830	29.863770
418.562237	17704.862956	29.868788
419.246490	17751.067146	29.873805
419.468214	17783.543038	29.878823
419.903159	17804.799257	29.883840
420.295963	17835.887647	29.888858
420.486849	17865.980767	29.893876
421.031667	17886.513333	29.898893
421.029360	17923.261798	29.903911
421.742533	17955.136347	29.908928
422.159287	17983.094991	29.913946
422.768038	18011.128996	29.918964
423.074122	18050.850538	29.923981
423.324684	18085.071014	29.928999
424.167085	18106.557206	29.934016
424.436952	18137.313833	29.939034
424.961397	18162.956911	29.944052
425.623128	18199.139615	29.949069
425.639907	18233.983082	29.954087
426.716177	18249.839078	29.959104
426.811011	18268.325013	29.964122
427.143648	18298.524337	29.969140
427.505815	18330.639440	29.974157
427.793485	18362.673962	29.979175
428.422362	18387.268906	29.984192
428.960309	18419.491223	29.989210
429.182383	18429.364329	29.994228
429.878672	18461.106395	29.999245
430.129216	18499.059617	30.004263
430.893017	18520.605760	30.009280
431.424598	18539.162587	30.014298
431.285922	18563.978135	30.019316
431.880572	18598.712239	30.024333
432.153904	18627.929142	30.029351
432.856260	18636.997122	30.034368
433.088885	18678.781573	30.039386
433.123982	18699.379895	30.044404
433.872343	18716.106729	30.049421
434.372116	18749.724005	30.054439
434.607654	18772.364116	30.059456
435.210514	18789.770514	30.064474
435.378495	18834.961370	30.069492
435.976483	18846.248482	30.074509
436.316806	18868.525973	30.079527
436.488943	18912.332126	30.084544
437.367858	18926.515521	30.089562
437.996201	18947.081072	30.094580
438.515058	18991.102289	30.099597
438.872656	19005.634569	30.104615
439.155752	19021.308676	30.109632
439.764828	19066.168504	30.114650
440.118307	19077.123474	30.119668
440.517924	19097.988272	30.124685
440.639713	19132.134719	30.129703
441.546152	19150.093960	30.134720
441.878123	19182.592813	30.139738
442.052298	19207.360721	30.144756
442.809416	19226.864362	30.149773
442.827382	19280.791725	30.154791
443.432788	19285.805311	30.159808
443.847057	19325.009314	30.164826
444.444203	19358.510029	30.169844
444.997489	19383.561925	30.174861
444.932155	19431.083120	30.179879
445.476928	19448.161703	30.184896
445.834886	19485.510427	30.189914
446.525890	19516.805869	30.194932
446.792356	19546.653183	30.199949
447.243455	19582.874643	30.204967
447.639661	19615.083834	30.209984
448.267934	19649.341283	30.215002
448.890162	19686.623187	30.220020
449.391271	19709.713327	30.225037
449.831394	19750.300591	30.230055
450.323149	19771.606368	30.235072
450.663394	19797.744914	30.240090
450.956750	19839.668875	30.245108
451.872843	19862.762031	30.250125
452.046703	19900.309989	30.255143
452.456658	19933.816172	30.260160
452.918456	19950.176187	30.265178
453.387553	19991.092951	30.270196
453.828815	20022.608349	30.275213
454.227295	20058.771575	30.280231
454.706017	20074.060428	30.285248
454.965166	20110.110133	30.290266
455.230406	20150.440053	30.295284
456.030363	20172.700126	30.300301
456.591514	20204.336960	30.305319
456.911903	20229.885636	30.310336
457.282071	20254.925980	30.315354
457.760338	20285.659165	30.320372
458.321663	20307.218004	30.325389
458.593676	20339.753233	30.330407
459.230634	20358.480903	30.335424
459.456824	20394.130959	30.340442
459.401397	20427.863542	30.345460
460.482563	20457.615878	30.350477
460.849007	20484.631026	30.355495
461.083163	20516.812377	30.360512
461.439070	20561.023848	30.365530
462.151427	20592.029828	30.370548
462.520375	20612.802711	30.375565
463.043821	20651.258704	30.380583
463.671308	20678.230237	30.385600
464.033049	20719.753882	30.390618
464.569080	20744.064952	30.395636
465.224233	20773.343566	30.400653
465.446451	20797.834259	30.405671
465.923615	20851.165460	30.410688
466.789278	20873.458201	30.415706
467.088916	20908.381879	30.420724
467.837949	20925.626030	30.425741
468.160737	20967.236075	30.430759
468.423998	20997.100845	30.435776
468.880505	21021.565982	30.440794
469.085846	21064.270744	30.445812
469.458104	21091.112365	30.450829
470.032671	21146.730979	30.455847
470.310142	21152.614480	30.460864
470.908990	21205.838511	30.465882
471.634409	21235.560018	30.470900
472.209425	21251.210338	30.475917
472.495091	21317.148903	30.480935
473.088347	21335.874079	30.485952
473.628522	21363.791175	30.490970
474.095218	21406.011455	30.495988
474.413654	21437.046427	30.501005
474.760814	21476.149172	30.506023
475.365952	21511.277930	30.511040
475.635207	21545.596340	30.516058
476.518551	21582.962453	30.521076
477.195945	21614.257971	30.526093
477.330251	21652.840632	30.531111
477.731882	21678.206649	30.536128
478.603870	21709.464269	30.541146
478.658346	21754.772205	30.546164
479.223000	21775.116163	30.551181
479.826170	21797.292957	30.556199
479.952474	21844.319182	30.561216
480.815883	21875.087063	30.566234
481.146897	21890.776107	30.571252
481.682053	21941.090925	30.576269
482.213600	21977.224780	30.581287
482.884308	22010.100435	30.586304
483.469838	22030.780841	30.591322
483.676460	22054.386026	30.596340
484.342768	22085.342446	30.601357
484.843842	22107.475300	30.606375
485.012216	22134.989118	30.611392
485.623888	22152.924766	30.616410
485.898869	22188.428965	30.621428
486.659289	22215.615487	30.626445
486.927020	22241.225053	30.631463
487.328600	22264.260004	30.636480
488.025933	22308.428304	30.641498
488.468158	22332.532717	30.646516
489.112135	22353.140444	30.651533
489.277484	22379.105992	30.656551
489.569071	22414.029179	30.661568
490.299102	22440.612915	30.666586
490.598178	22488.762631	30.671604
491.302662	22528.267083	30.676621
491.860365	22558.000488	30.681639
492.412721	22594.611304	30.686656
493.062510	22601.530801	30.691674
493.277907	22658.546954	30.696692
493.931835	22676.399285	30.701709
493.975338	22713.778225	30.706727
495.041633	22749.317514	30.711744
495.393606	22771.389993	30.716762
495.736384	22802.482062	30.721780
496.220412	22849.283386	30.726797
496.716535	22878.990190	30.731815
497.181868	22911.127011	30.736832
497.818279	22934.667412	30.741850
498.031279	22983.045001	30.746868
498.823742	23021.989284	30.751885
499.241944	23033.410870	30.756903
499.646311	23095.281728	30.761920
500.358570	23113.256009	30.766938
500.624500	23160.068579	30.771956
501.587098	23185.731238	30.776973
501.997364	23219.021091	30.781991
502.215831	23260.356483	30.787008
502.823474	23296.809683	30.792026
503.270139	23305.667920	30.797044
503.741623	23372.749594	30.802061
504.017795	23390.542404	30.807079
504.782829	23424.418887	30.812096
505.299931	23467.848048	30.817114
505.619376	23509.765035	30.822132
505.971266	23530.781574	30.827149
506.787947	23569.965945	30.832167
506.875821	23624.898941	30.837184
508.006979	23640.956126	30.842202
507.837794	23699.599982	30.847220
508.568110	23722.229465	30.852237
509.105535	23793.863712	30.857255
509.759700	23795.510478	30.862272
510.063412	23862.512252	30.867290
510.648473	23864.439412	30.872308
511.060264	23927.407182	30.877325
511.345539	23930.204425	30.882343
512.079015	23981.249519	30.887360
512.509448	23998.779777	30.892378
513.055030	24018.765775	30.897396
513.668664	24069.567163	30.902413
514.339089	24101.901371	30.907431
514.631249	24129.907775	30.912448
515.198164	24187.618571	30.917466
515.837435	24210.651582	30.922484
516.641738	24247.801097	30.927501
516.926077	24270.464598	30.932519
517.008187	24337.831350	30.937536
517.600428	24332.613934	30.942554
518.047974	24413.937251	30.947572
518.484429	24422.373968	30.952589
518.752839	24479.009341	30.957607
519.653689	24503.832491	30.962624
520.219194	24540.370097	30.967642
520.504791	24599.230755	30.972660
521.344650	24630.474087	30.977677
521.888528	24653.101519	30.982695
522.313486	24724.441220	30.987712
522.844965	24737.599422	30.992730
523.386664	24786.884055	30.997748
523.634873	24853.256074	31.002765
524.694747	24876.790994	31.007783
524.831492	24933.885347	31.012800
525.765447	24957.765771	31.017818
526.126128	24999.955031	31.022836
526.881699	25039.775853	31.027853
527.625293	25075.631728	31.032871
527.923803	25111.269487	31.037888
528.665591	25131.440683	31.042906
529.408514	25170.786489	31.047924
529.935009	25206.288892	31.052941
530.364607	25219.034413	31.057959
530.490470	25256.992280	31.062976
531.392722	25300.709340	31.067994
531.392488	25328.201988	31.073012
532.371532	25374.770424	31.078029
533.093893	25409.670187	31.083047
532.888666	25439.324927	31.088064
533.862032	25490.828993	31.093082
534.518122	25515.557224	31.098100
534.648591	25544.086572	31.103117
535.131798	25602.201032	31.108135
535.919183	25634.455135	31.113152
536.599835	25660.079286	31.118170
536.842519	25711.519268	31.123188
537.224812	25764.024277	31.128205
538.097642	25778.661941	31.133223
538.408140	25824.440139	31.138240
538.963162	25846.271073	31.143258
539.594345	25897.718308	31.148276
539.933913	25915.431373	31.153293
540.947225	25926.158413	31.158311
541.051112	26006.035228	31.163328
541.842641	25986.596329	31.168346
541.975166	26072.240073	31.173364
542.320483	26092.312573	31.178381
543.299761	26137.429766	31.183399
543.794830	26172.709295	31.188416
544.344119	26202.034142	31.193434
544.935512	26227.786074	31.198452
545.381842	26277.933421	31.203469
546.202145	26312.025479	31.208487
546.158481	26343.876120	31.213504
547.042935	26377.863566	31.218522
547.501768	26417.683100	31.223540
548.116000	26453.095521	31.228557
548.872600	26481.728484	31.233575
549.027795	26528.124270	31.238592
549.864132	26557.621479	31.243610
550.233894	26619.344518	31.248628
550.869954	26648.743020	31.253645
551.180089	26691.436379	31.258663
551.353642	26733.372469	31.263680
551.926964	26789.012641	31.268698
552.803872	26805.000901	31.273716
553.124057	26870.573346	31.278733
554.065543	26939.896344	31.283751
554.133897	26959.336527	31.288768
555.326555	26982.405947	31.293786
555.842694	27066.950827	31.298804
556.544643	27082.595383	31.303821
557.083094	27140.717651	31.308839
557.417714	27161.085475	31.313856
558.014568	27220.446639	31.318874
558.371162	27243.165875	31.323892
558.737604	27302.588462	31.328909
559.873376	27354.147506	31.333927
560.354154	27385.371498	31.338944
560.767428	27427.925906	31.343962
561.516328	27469.571380	31.348980
562.128480	27508.242591	31.353997
562.947530	27549.316158	31.359015
563.239190	27596.696997	31.364032
564.020508	27612.601238	31.369050
564.379627	27638.895866	31.374068
564.694502	27697.814449	31.379085
565.700429	27720.030713	31.384103
566.268803	27766.065664	31.389120
566.952228	27797.571746	31.394138
567.375885	27840.407641	31.399156
568.261322	27863.300366	31.404173
568.806812	27891.171374	31.409191
568.765001	27939.875571	31.414208
569.774751	27950.202751	31.419226
570.359156	28001.476667	31.424244
570.658197	28030.326300	31.429261
571.249243	28049.419827	31.434279
571.770892	28082.702869	31.439296
572.086209	28131.149069	31.444314
572.518509	28165.833163	31.449332
573.187268	28175.362322	31.454349
573.802060	28248.226167	31.459367
574.233647	28258.185512	31.464384
574.910932	28331.022443	31.469402
575.137542	28357.774258	31.474420
575.662867	28410.097307	31.479437
576.273025	28453.125732	31.484455
576.778790	28501.903562	31.489472
577.500319	28550.749601	31.494490
577.946580	28601.187047	31.499508
578.614782	28642.334701	31.504525
579.321432	28694.073537	31.509543
579.965501	28737.377809	31.514560
580.586530	28768.884697	31.519578
581.160388	28806.716555	31.524596
581.564400	28848.660044	31.529613
582.866806	28900.066710	31.534631
583.031127	28940.085148	31.539648
583.536632	28984.382852	31.544666
584.237894	29032.034373	31.549684
584.839004	29065.480126	31.554701
585.527343	29127.804957	31.559719
585.929064	29172.014122	31.564736
586.420793	29206.470365	31.569754
587.208486	29248.583856	31.574772
587.774023	29302.756581	31.579789
588.449188	29333.436505	31.584807
588.725233	29389.820849	31.589824
589.122169	29431.461255	31.594842
590.057140	29481.573046	31.599860
590.614990	29525.285548	31.604877
591.012246	29563.991967	31.609895
591.425832	29605.002968	31.614912
592.204342	29664.767301	31.619930
593.352817	29722.132735	31.624948
593.378299	29773.373628	31.629965
594.122652	29806.227622	31.634983
594.552742	29859.133110	31.640000
595.105800	29905.219135	31.645018
595.709664	29946.867304	31.650036
596.091529	30005.230458	31.655053
596.918403	30059.379844	31.660071
597.347031	30105.908600	31.665088
598.181049	30155.393994	31.670106
599.031328	30201.151430	31.675124
599.563916	30248.776651	31.680141
600.377437	30288.769086	31.685159
600.770317	30342.761594	31.690176
601.454537	30367.205991	31.695194
601.991808	30404.064004	31.700212
602.351932	30441.301751	31.705229
603.173912	30473.422943	31.710247
603.526991	30523.799247	31.715264
603.995354	30554.421432	31.720282
604.978728	30606.368145	31.725300
605.199815	30644.033523	31.730317
605.756692	30683.178946	31.735335
606.336851	30732.544196	31.740352
606.851681	30782.533061	31.745370
607.673830	30826.739654	31.750388
607.899674	30883.026836	31.755405
608.901440	30926.825278	31.760423
609.664495	30978.207804	31.765440
610.196144	31039.624029	31.770458
610.835171	31063.764619	31.775476
611.377324	31109.272656	31.780493
611.616076	31177.982614	31.785511
612.773522	31203.586940	31.790528
613.263919	31252.520462	31.795546
613.813529	31300.272124	31.800564
614.311883	31361.748446	31.805581
615.260608	31401.149975	31.810599
615.897499	31459.305921	31.815616
616.369042	31504.856248	31.820634
617.000306	31560.482291	31.825652
617.755242	31588.583199	31.830669
618.042217	31651.879961	31.835687
618.562718	31704.420834	31.840704
619.211824	31755.163568	31.845722
620.175819	31792.388608	31.850740
620.582523	31853.818326	31.855757
621.591952	31898.459792	31.860775
621.916436	31956.585295	31.865792
622.945184	31999.025289	31.870810
623.354788	32052.385602	31.875828
623.993813	32092.618293	31.880845
624.805447	32140.633293	31.885863
625.514923	32192.184199	31.890880
625.746407	32236.293224	31.895898
626.473670	32286.727267	31.900916
627.002653	32337.539792	31.905933
627.664114	32377.011483	31.910951
628.262161	32425.256770	31.915968
628.887036	32480.819176	31.920986
629.488399	32537.577092	31.926004
629.876933	32583.545553	31.931021
630.552685	32625.981913	31.936039
631.417851	32679.035288	31.941056
632.278579	32732.674304	31.946074
632.785862	32777.051366	31.951092
633.155247	32833.602935	31.956109
634.111452	32871.726945	31.961127
634.964799	32907.061791	31.966144
635.000613	32952.516865	31.971162
635.931711	32994.267272	31.976180
636.337080	33031.978136	31.981197
636.932822	33088.701019	31.986215
637.389677	33127.114775	31.991232
638.166664	33169.955692	31.996250
638.750496	33222.601667	32.001268
639.123754	33280.692551	32.006285
640.005268	33323.826165	32.011303
640.692281	33378.801650	32.016320
641.088396	33425.636608	32.021338
642.037265	33468.819775	32.026356
642.173766	33511.766723	32.031373
643.010981	33566.709458	32.036391
643.886789	33629.601647	32.041408
644.434368	33685.561879	32.046426
645.222907	33723.265324	32.051444
645.927164	33782.906762	32.056461
646.552514	33820.669518	32.061479
647.171180	33879.632944	32.066496
647.345156	33949.446107	32.071514
648.484670	33990.418687	32.076532
649.075129	34041.707444	32.081549
649.681674	34100.607383	32.086567
650.302162	34151.915344	32.091584
651.039443	34200.922354	32.096602
651.684009	34246.509460	32.101620
652.466031	34310.147433	32.106637
652.993484	34343.771763	32.111655
654.126716	34406.641680	32.116672
654.205272	34474.678372	32.121690
655.270285	34511.776837	32.126708
655.844625	34560.479824	32.131725
656.385440	34621.851194	32.136743
656.992292	34669.272470	32.141760
657.195962	34724.870083	32.146778
658.274962	34774.024575	32.151796
659.178862	34840.030231	32.156813
659.320480	34887.559314	32.161831
660.205040	34939.828670	32.166848
660.733038	35008.349292	32.171866
661.239746	35058.699232	32.176884
662.035269	35120.427563	32.181901
662.617453	35172.055330	32.186919
663.453598	35233.750814	32.191936
664.151158	35293.859065	32.196954
664.938226	35346.285525	32.201972
665.606748	35395.048476	32.206989
666.884544	35448.175879	32.212007
667.607500	35494.438104	32.217024
668.042149	35543.301786	32.222042
668.713023	35597.137966	32.227060
669.251856	35652.991140	32.232077
669.774344	35702.858119	32.237095
670.436519	35741.596793	32.242112
670.940301	35790.292544	32.247130
671.929191	35831.000441	32.252148
672.220787	35885.046130	32.257165
672.773821	35929.247782	32.262183
673.438421	35975.408704	32.267200
673.706769	36031.470168	32.272218
674.547887	36063.603966	32.277236
675.367666	36130.539349	32.282253
675.920575	36171.260743	32.287271
676.364552	36226.951219	32.292288
676.969771	36297.910012	32.297306
677.912008	36342.946252	32.302324
678.569974	36418.883705	32.307341
679.136900	36482.679320	32.312359
679.900255	36531.812016	32.317376
680.341169	36590.934745	32.322394
681.308683	36653.073338	32.327412
681.930493	36716.156384	32.332429
682.510228	36790.094711	32.337447
683.456041	36835.927876	32.342464
683.949725	36898.776606	32.347482
685.102683	36958.025320	32.352500
685.521517	37017.414780	32.357517
686.240795	37075.567863	32.362535
687.257183	37119.088743	32.367552
688.141850	37180.113641	32.372570
688.690654	37239.445354	32.377588
689.388673	37292.927935	32.382605
690.090035	37340.121028	32.387623
690.913921	37384.997608	32.392640
691.453105	37444.161301	32.397658
692.262766	37494.610663	32.402676
692.790754	37560.906079	32.407693
693.480549	37607.198350	32.412711
694.630146	37650.757740	32.417728
694.793036	37711.653531	32.422746
695.887659	37764.703956	32.427764
696.711483	37830.649039	32.432781
697.212363	37861.762030	32.437799
697.971632	37918.486359	32.442816
698.250754	37979.230594	32.447834
699.311023	38025.316825	32.452852
699.951123	38087.899150	32.457869
700.407841	38140.418497	32.462887
701.606645	38201.802300	32.467904
701.443147	38255.220136	32.472922
702.283931	38315.213941	32.477940
703.333742	38371.046845	32.482957
703.690404	38431.220628	32.487975
704.194816	38479.171987	32.492992
704.940236	38542.180711	32.498010
705.742240	38620.363052	32.503028
706.741659	38668.918867	32.508045
707.265479	38726.859651	32.513063
708.038586	38779.940815	32.518080
708.856446	38835.361235	32.523098
709.249999	38888.884745	32.528116
709.891669	38945.478306	32.533133
710.382535	38991.845473	32.538151
711.099638	39039.980579	32.543168
711.872017	39110.199303	32.548186
712.789444	39169.848088	32.553204
713.382593	39229.845149	32.558221
713.555689	39307.317166	32.563239
714.363631	39343.365117	32.568256
715.285539	39413.480874	32.573274
715.895886	39489.278915	32.578292
716.699207	39556.962195	32.583309
717.498268	39608.958551	32.588327
717.992142	39681.579763	32.593344
718.980078	39723.071486	32.598362
719.874412	39817.792011	32.603380
720.550434	39848.265809	32.608397
721.161222	39945.588264	32.613415
721.402433	39977.716262	32.618432
722.254932	40057.089301	32.623450
723.027353	40128.583190	32.628468
723.890158	40192.358341	32.633485
724.625030	40297.377163	32.638503
725.429921	40336.926838	32.643520
726.475729	40392.970473	32.648538
727.174149	40465.865233	32.653556
728.131066	40516.314367	32.658573
728.352008	40607.481750	32.663591
729.772757	40639.446867	32.668608
730.164625	40730.092539	32.673626
731.159208	40778.890139	32.678644
731.864612	40820.322294	32.683661
732.718273	40912.816133	32.688679
733.866144	40948.464874	32.693696
734.262065	40991.143622	32.698714
734.854448	41083.232124	32.703732
735.631008	41114.114814	32.708749
736.103345	41172.715537	32.713767
736.859708	41231.750645	32.718784
737.396877	41320.130699	32.723802
738.139138	41352.542651	32.728820
739.288074	41448.193670	32.733837
740.084537	41477.272919	32.738855
741.075401	41551.518252	32.743872
741.547046	41621.046134	32.748890
742.073664	41660.211083	32.753908
743.291150	41744.369007	32.758925
743.683042	41778.430341	32.763943
745.153996	41836.751356	32.768960
745.743973	41895.641771	32.773978
746.455826	41949.586300	32.778996
747.437600	41995.833033	32.784013
747.638571	42042.238886	32.789031
748.486225	42099.691713	32.794048
749.165258	42157.843406	32.799066
749.724224	42197.281996	32.804084
750.496276	42228.981191	32.809101
750.746197	42299.701537	32.814119
751.470577	42360.559269	32.819136
752.045771	42412.353790	32.824154
752.718163	42481.827970	32.829172
753.735529	42539.463430	32.834189
754.109434	42604.522434	32.839207
754.922658	42657.585645	32.844224
755.733679	42737.384629	32.849242
756.509103	42797.267433	32.854260
757.589930	42860.968945	32.859277
757.965556	42932.056697	32.864295
758.793787	42989.502977	32.869312
759.776204	43055.851546	32.874330
760.638789	43126.509301	32.879348
761.389273	43186.066226	32.884365
762.045982	43257.224129	32.889383
762.980089	43310.636013	32.894400
763.503327	43380.913532	32.899418
764.353462	43456.933866	32.904436
765.130387	43497.391146	32.909453
765.949243	43583.889536	32.914471
766.467833	43636.608369	32.919488
767.389351	43705.451645	32.924506
768.422717	43775.961853	32.929524
769.193781	43833.956300	32.934541
769.672110	43913.226961	32.939559
770.626933	43974.735074	32.944576
771.430454	44041.434514	32.949594
772.002143	44113.458030	32.954612
773.031917	44171.002343	32.959629
773.500606	44242.743115	32.964647
774.596948	44310.248696	32.969664
775.630502	44381.796029	32.974682
776.269762	44443.807141	32.979700
777.318024	44505.403214	32.984717
777.989609	44565.236128	32.989735
778.894353	44618.997428	32.994752
779.497177	44685.762844	32.999770
780.247912	44761.120186	33.004788
780.872995	44820.024464	33.009805
781.755239	44879.591487	33.014823
782.544125	44942.722540	33.019840
783.359788	45012.076831	33.024858
784.002301	45074.146463	33.029876
785.118613	45138.623622	33.034893
785.455397	45226.837913	33.039911
786.392050	45281.586759	33.044928
787.229334	45340.383311	33.049946
787.485847	45428.333784	33.054964
788.721690	45489.058027	33.059981
789.121724	45555.332220	33.064999
789.777262	45626.033131	33.070016
790.625629	45685.311761	33.075034
791.249212	45760.116348	33.080052
792.372207	45820.724055	33.085069
792.708243	45881.785338	33.090087
793.395196	45956.634312	33.095104
794.157382	46029.550339	33.100122
794.696655	46097.908701	33.105140
795.782790	46151.614321	33.110157
796.288569	46233.790497	33.115175
797.273403	46324.024094	33.120192
797.732182	46377.681990	33.125210
798.440761	46470.294935	33.130228
799.709935	46558.260271	33.135245
800.469772	46633.567470	33.140263
801.202022	46716.198878	33.145280
802.099330	46787.645280	33.150298
802.790112	46864.163350	33.155316
803.820844	46945.274952	33.160333
804.682581	47016.462929	33.165351
805.483629	47083.559329	33.170368
806.564787	47174.504477	33.175386
807.191771	47259.060840	33.180404
808.604896	47317.472662	33.185421
809.181389	47392.342199	33.190439
810.182500	47453.148500	33.195456
810.746596	47523.414142	33.200474
811.209761	47602.524136	33.205492
812.082577	47681.635539	33.210509
813.118887	47766.731822	33.215527
813.951884	47839.691437	33.220544
814.540452	47913.548465	33.225562
815.459435	47989.249476	33.230580
816.727955	48052.612005	33.235597
817.666969	48133.702677	33.240615
818.194430	48202.878849	33.245632
819.342324	48272.934665	33.250650
819.915929	48342.406942	33.255668
820.669519	48427.371567	33.260685
821.758445	48485.816793	33.265703
822.465780	48564.523073	33.270720
823.383559	48631.054621	33.275738
824.014748	48706.911801	33.280756
825.027813	48769.494033	33.285773
825.798703	48850.466458	33.290791
826.510735	48912.238858	33.295808
827.356040	48990.092061	33.300826
827.532781	49082.052420	33.305844
828.876309	49148.963064	33.310861
829.221628	49233.072011	33.315879
830.619694	49310.986953	33.320896
831.674548	49383.005720	33.325914
831.988370	49466.814712	33.330932
833.276788	49531.078689	33.335949
833.998175	49610.768730	33.340967
834.855017	49676.149539	33.345984
835.817033	49737.383308	33.351002
836.408492	49805.791930	33.356020
837.150860	49868.503176	33.361037
837.935537	49929.936232	33.366055
838.674847	49996.062697	33.371072
839.385663	50063.487720	33.376090
840.302736	50133.745422	33.381108
841.187287	50197.858362	33.386125
841.981501	50281.834561	33.391143
842.717886	50349.966608	33.396160
843.885420	50427.566565	33.401178
844.609782	50488.064465	33.406196
845.340379	50563.759134	33.411213
846.013421	50636.739955	33.416231
847.337341	50700.402945	33.421248
848.279382	50785.891647	33.426266
848.889187	50854.929360	33.431284
849.745850	50924.436121	33.436301
850.928758	51002.247569	33.441319
851.425072	51074.494624	33.446336
852.604570	51143.947705	33.451354
853.064349	51219.820799	33.456372
853.580847	51308.311424	33.461389
855.026167	51371.714499	33.466407
855.691467	51450.348729	33.471424
856.585607	51517.349287	33.476442
857.037044	51603.421753	33.481460
858.136699	51679.359061	33.486477
858.964361	51765.801625	33.491495
859.697797	51852.111276	33.496512
860.822806	51930.324150	33.501530
861.531882	52010.440291	33.506548
862.657403	52086.671864	33.511565
863.702897	52162.203260	33.516583
864.409049	52244.312297	33.521600
864.982548	52331.523900	33.526618
866.275816	52403.744159	33.531636
867.201957	52487.675005	33.536653
868.065987	52558.534540	33.541671
868.882620	52643.310409	33.546688
870.306667	52704.717532	33.551706
870.878108	52781.538885	33.556724
871.368833	52848.829539	33.561741
872.229768	52933.047415	33.566759
873.140971	53016.269835	33.571776
874.356183	53084.907335	33.576794
874.854124	53167.161023	33.581812
875.818190	53239.317099	33.586829
876.937618	53321.283220	33.591847
877.456961	53410.553831	33.596864
878.571468	53481.516007	33.601882
879.107715	53562.436659	33.606900
879.794804	53635.370627	33.611917
881.034606	53730.922587	33.616935
882.041830	53790.745904	33.621952
882.788400	53865.997461	33.626970
883.357928	53940.879819	33.631988
884.625215	53991.146378	33.637005
885.670991	54056.677238	33.642023
886.075520	54146.225406	33.647040
886.966117	54211.538489	33.652058
887.913602	54278.155771	33.657076
888.747561	54347.976074	33.662093
889.629776	54426.017481	33.667111
890.328058	54507.961311	33.672128
891.325906	54585.801938	33.677146
892.103697	54671.751881	33.682164
893.134280	54744.379987	33.687181
893.920915	54821.876472	33.692199
894.487747	54918.179376	33.697216
895.645426	54991.741480	33.702234
896.481979	55079.893492	33.707252
897.012869	55159.196555	33.712269
898.073264	55244.637081	33.717287
898.839766	55342.829582	33.722304
900.309256	55418.471258	33.727322
900.710312	55515.826402	33.732340
901.902933	55601.850455	33.737357
902.961423	55680.383707	33.742375
903.684528	55769.201038	33.747392
904.823267	55858.034733	33.752410
905.488254	55951.123558	33.757428
906.616071	56025.720480	33.762445
907.511982	56121.415494	33.767463
908.542045	56204.886151	33.772480
909.655807	56286.033211	33.777498
910.172020	56387.664542	33.782516
910.925376	56471.385628	33.787533
912.276994	56563.152988	33.792551
912.989076	56642.875592	33.797568
914.391419	56713.283733	33.802586
915.208660	56805.011069	33.807604
916.151005	56895.771934	33.812621
917.031938	56976.059429	33.817639
917.786315	57055.833919	33.822656
918.675704	57144.281056	33.827674
919.658552	57239.039976	33.832692
920.618246	57317.125609	33.837709
921.991805	57390.599888	33.842727
922.337787	57474.147293	33.847744
923.309442	57561.257472	33.852762
924.210606	57645.484429	33.857780
925.247578	57735.959737	33.862797
925.981771	57827.904273	33.867815
926.867426	57908.542346	33.872832
927.789785	57990.279857	33.877850
928.425741	58089.341264	33.882868
929.315376	58190.478002	33.887885
930.614028	58256.179428	33.892903
931.595903	58343.313775	33.897920
932.466524	58420.291211	33.902938
933.759726	58493.066038	33.907956
934.489247	58577.378229	33.912973
935.189484	58657.376628	33.917991
936.118772	58739.188963	33.923008
936.989707	58802.179023	33.928026
937.823793	58898.204550	33.933044
938.351893	58986.335996	33.938061
939.769937	59072.220463	33.943079
940.476316	59155.285592	33.948096
941.388293	59246.129151	33.953114
942.335043	59336.074146	33.958132
943.159304	59418.073518	33.963149
944.313286	59515.191077	33.968167
945.192482	59609.517695	33.973184
946.475708	59677.884996	33.978202
947.060501	59773.872628	33.983220
948.112479	59871.494493	33.988237
949.353711	59951.140866	33.993255
949.958900	60046.451003	33.998272
951.015753	60140.423688	34.003290
951.984596	60231.528225	34.008308
952.751239	60326.956186	34.013325
953.949584	60414.940396	34.018343
954.633225	60513.476711	34.023360
956.006979	60594.626597	34.028378
956.889912	60705.613311	34.033396
957.910164	60798.420585	34.038413
958.826238	60880.790673	34.043431
959.798406	60965.103495	34.048448
960.868667	61052.454342	34.053466
961.542946	61164.619972	34.058484
962.657256	61248.134716	34.063501
963.791915	61336.588076	34.068519
964.532073	61443.285581	34.073536
965.640439	61521.668372	34.078554
966.575669	61612.709206	34.083572
967.603109	61716.943880	34.088589
968.340706	61807.830808	34.093607
969.345505	61904.469842	34.098624
970.724604	62004.895788	34.103642
971.634563	62096.062974	34.108660
972.723375	62187.524225	34.113677
973.733151	62266.813110	34.118695
974.626078	62376.421906	34.123712
975.817119	62463.466440	34.128730
976.745214	62562.356698	34.133748
977.410522	62642.630334	34.138765
978.862351	62725.482194	34.143783
979.697942	62823.371749	34.148800
980.417559	62912.018548	34.153818
981.666401	62987.410490	34.158836
982.323012	63101.867227	34.163853
983.572661	63178.532394	34.168871
984.282979	63259.723570	34.173888
985.364690	63343.000175	34.178906
986.471402	63416.158592	34.183924
986.893883	63528.387823	34.188941
987.940150	63581.545128	34.193959
988.771662	63682.629228	34.198976
989.665787	63768.397544	34.203994
990.342898	63846.928091	34.209012
991.462006	63962.418556	34.214029
992.537201	64030.383241	34.219047
993.514710	64152.026961	34.224064
994.757847	64225.782604	34.229082
995.679202	64311.056395	34.234100
996.670871	64427.318404	34.239117
997.984488	64505.946210	34.244135
999.007255	64599.785518	34.249152
999.755202	64691.935237	34.254170
1000.934728	64787.547466	34.259188
1001.780123	64881.918515	34.264205
1002.847027	64980.464544	34.269223
1003.503514	65082.341870	34.274240
1004.868748	65167.975228	34.279258
1005.848019	65277.852333	34.284276
1006.738408	65384.273379	34.289293
1007.906067	65483.785009	34.294311
1009.067506	65580.405234	34.299328
1009.710665	65670.460347	34.304346
1010.840658	65791.932354	34.309364
1011.722759	65861.630266	34.314381
1012.872274	65968.970289	34.319399
1013.881316	66086.262909	34.324416
1015.262177	66171.212928	34.329434
1016.258099	66283.742968	34.334452
1017.066992	66377.460793	34.339469
1018.088714	66471.893747	34.344487
1019.289932	66578.082472	34.349504
1020.083089	66672.236933	34.354522
1021.210090	66781.739098	34.359540
1022.392529	66884.973085	34.364557
1023.455276	66974.057937	34.369575
1024.125536	67084.847321	34.374592
1025.323988	67182.982621	34.379610
1026.696098	67284.470371	34.384628
1027.465166	67373.872260	34.389645
1028.683116	67483.840879	34.394663
1029.747347	67555.957494	34.399680
1030.630033	67691.589976	34.404698
1031.460057	67750.971411	34.409716
1032.792846	67878.833043	34.414733
1034.107668	67964.853294	34.419751
1034.911283	68060.582684	34.424768
1035.774988	68181.856273	34.429786
1037.228469	68245.972754	34.434804
1038.110768	68383.511642	34.439821
1038.790067	68446.191559	34.444839
1040.180620	68514.412578	34.449856
1041.071891	68642.709573	34.454874
1041.860668	68707.324997	34.459892
1042.971000	68807.229323	34.464909
1043.717348	68892.352278	34.469927
1044.781470	68965.447053	34.474944
1045.534049	69102.834774	34.479962
1046.219603	69183.243141	34.484980
1047.693413	69285.833936	34.489997
1048.318807	69383.386076	34.495015
1049.666828	69476.110769	34.500032
1050.477953	69595.784211	34.505050
1051.979957	69680.411346	34.510068
1052.856236	69813.052401	34.515085
1054.205899	69901.514352	34.520103
1054.878357	70010.478428	34.525120
1056.152815	70125.317754	34.530138
1057.099313	70211.457078	34.535156
1058.056102	70350.495333	34.540173
1059.734817	70453.779921	34.545191
1060.482327	70550.257032	34.550208
1061.790821	70622.870567	34.555226
1062.696363	70751.387637	34.560244
1063.619871	70839.738391	34.565261
1065.234643	70946.858211	34.570279
1066.374634	71049.656679	34.575296
1067.135840	71142.103519	34.580314
1068.275674	71264.293737	34.585332
1069.070550	71356.338178	34.590349
1070.209670	71478.403472	34.595367
1071.535357	71551.036662	34.600384
1072.475836	71701.390582	34.605402
1073.787518	71768.131744	34.610420
1074.687663	71906.817221	34.615437
1076.106424	72003.864446	34.620455
1076.909678	72099.335641	34.625472
1077.591395	72227.790523	34.630490
1079.249702	72298.844474	34.635508
1079.999019	72433.494787	34.640525
1081.271691	72530.460418	34.645543
1082.301072	72641.878149	34.650560
1083.410575	72746.067779	34.655578
1084.773226	72853.617184	34.660596
1085.493952	72981.660026	34.665613
1086.586903	73060.989485	34.670631
1088.139075	73152.340503	34.675648
1089.168311	73291.217338	34.680666
1090.215645	73370.599523	34.685684
1091.297337	73465.818167	34.690701
1092.354512	73589.558755	34.695719
1093.460545	73667.056047	34.700736
1094.611146	73793.677153	34.705754
1095.641245	73880.729131	34.710772
1096.704620	74003.156931	34.715789
1098.170737	74091.783455	34.720807
1098.999001	74175.507033	34.725824
1099.813081	74298.007887	34.730842
1101.267600	74346.870606	34.735860
1101.840260	74474.150360	34.740877
1103.186500	74534.051572	34.745895
1103.960677	74676.940811	34.750912
1104.855439	74753.161502	34.755930
1106.129611	74847.010101	34.760948
1106.700935	74968.947006	34.765965
1108.135544	75062.290820	34.770983
1108.953450	75170.451239	34.776000
1109.825101	75281.744496	34.781018
1111.325285	75378.858431	34.786036
1112.167811	75525.047962	34.791053
1113.376373	75625.223919	34.796071
1114.189339	75777.341479	34.801088
1115.256943	75873.243706	34.806106
1116.840566	75977.355822	34.811124
1117.555908	76118.798482	34.816141
1119.261003	76195.066402	34.821159
1120.325677	76344.854118	34.826176
1121.492347	76436.407847	34.831194
1122.874600	76579.713153	34.836212
1123.763472	76653.957525	34.841229
1124.891761	76814.823807	34.846247
1126.050231	76888.621684	34.851264
1127.128325	77031.751042	34.856282
1128.613481	77121.089436	34.861300
1129.818278	77238.945005	34.866317
1130.906086	77379.136406	34.871335
1132.187591	77459.199056	34.876352
1132.841187	77556.066254	34.881370
1134.196476	77712.643714	34.886388
1135.544760	77807.631953	34.891405
1136.638740	77937.315544	34.896423
1137.647299	78034.084323	34.901440
1139.295984	78126.479165	34.906458
1140.228957	78271.751348	34.911476
1141.326110	78399.162008	34.916493
1142.535161	78470.018560	34.921511
1144.092761	78614.707169	34.926528
1144.949537	78707.565572	34.931546
1145.892896	78836.551962	34.936564
1147.348271	78939.252258	34.941581
1148.280506	79052.402203	34.946599
1149.569728	79165.496003	34.951616
1150.383720	79278.786095	34.956634
1152.002155	79381.462679	34.961652
1152.685503	79498.244878	34.966669
1154.086873	79605.716693	34.971687
1155.339705	79741.934883	34.976704
1156.643826	79843.064572	34.981722
1157.477685	79942.379570	34.986740
1158.629283	80073.976466	34.991757
1159.831317	80162.513547	34.996775
1161.109235	80265.134923	35.001792
1161.691603	80387.431233	35.006810
1163.371666	80460.552259	35.011828
1164.098567	80588.010100	35.016845
1165.395232	80672.792196	35.021863
1166.794032	80783.759872	35.026880
1167.743989	80890.045930	35.031898
1168.552582	80983.921035	35.036916
1169.572858	81113.971443	35.041933
1171.033762	81193.280574	35.046951
1172.375285	81340.494371	35.051968
1173.221478	81418.201659	35.056986
1174.773072	81551.590214	35.062004
1175.963969	81631.304284	35.067021
1176.962510	81760.420302	35.072039
1178.462588	81866.339421	35.077056
1179.495689	81970.910980	35.082074
1180.649136	82093.234011	35.087092
1181.998625	82184.695860	35.092109
1183.169128	82302.206630	35.097127
1184.544232	82413.566099	35.102144
1185.401989	82517.725766	35.107162
1187.022370	82638.523749	35.112180
1188.416003	82742.871168	35.117197
1189.035492	82849.276692	35.122215
1190.557314	82974.966446	35.127232
1191.627157	83065.401906	35.132250
1192.721197	83206.270466	35.137268
1193.970243	83314.247248	35.142285
1194.870696	83424.840437	35.147303
1196.016216	83545.807680	35.152320
1197.196595	83678.206762	35.157338
1198.608697	83785.009420	35.162356
1199.287687	83905.104594	35.167373
1200.490508	84046.163805	35.172391
1201.778151	84169.280561	35.177408
1203.285750	84298.849733	35.182426
1204.180057	84404.656759	35.187444
1205.444103	84558.025552	35.192461
1206.863253	84654.911715	35.197479
1208.152217	84779.833713	35.202496
1209.300241	84913.876899	35.207514
1210.757556	85033.917972	35.212532
1211.836437	85154.165318	35.217549
1213.076355	85273.799741	35.222567
1214.806802	85381.571492	35.227584
1215.737361	85528.323671	35.232602
1217.051851	85630.156300	35.237620
1218.056038	85750.621234	35.242637
1219.367382	85876.406038	35.247655
1220.693638	85998.768582	35.252672
1221.648532	86118.604838	35.257690
1223.241080	86237.821909	35.262708
1224.627050	86357.489806	35.267725
1225.717925	86459.753989	35.272743
1227.046425	86560.905978	35.277760
1228.068304	86665.192820	35.282778
1229.404759	86768.538610	35.287796
1230.638568	86866.811161	35.292813
1231.383523	86968.171678	35.297831
1232.959501	87078.088511	35.302848
1233.671733	87190.748376	35.307866
1234.907519	87303.388825	35.312884
1236.332370	87414.387387	35.317901
1237.080736	87522.990074	35.322919
1238.197620	87629.878021	35.327936
1239.575721	87767.285555	35.332954
1240.876620	87882.681990	35.337972
1241.973066	88009.468360	35.342989
1243.087989	88134.222719	35.348007
1244.649266	88256.137160	35.353024
1245.336472	88390.142676	35.358042
1247.075137	88515.799195	35.363060
1248.561428	88639.574206	35.368077
1249.404680	88768.258107	35.373095
1251.011495	88890.497730	35.378112
1252.428496	89009.966831	35.383130
1253.904379	89129.218549	35.388148
1254.948454	89265.714900	35.393165
1256.325333	89381.164199	35.398183
1257.746506	89493.786646	35.403200
1258.843917	89623.668377	35.408218
1260.568377	89746.419021	35.413236
1261.615645	89865.806181	35.418253
1262.463911	89996.305231	35.423271
1264.092911	90119.174345	35.428288
1265.454221	90236.123140	35.433306
1266.596885	90358.723104	35.438324
1268.082052	90480.232154	35.443341
1269.333968	90604.182141	35.448359
1270.927661	90741.751389	35.453376
1271.815261	90867.752911	35.458394
1273.057788	90984.977582	35.463412
1274.333427	91097.163482	35.468429
1275.371576	91239.200594	35.473447
1276.730888	91363.074574	35.478464
1277.854769	91490.193156	35.483482
1279.567883	91610.141756	35.488500
1280.464876	91732.516538	35.493517
1281.850080	91884.609174	35.498535
1283.279520	91978.971635	35.503552
1284.166243	92141.669340	35.508570
1285.841302	92251.425936	35.513588
1287.101601	92372.842110	35.518605
1288.377915	92521.926956	35.523623
1289.499160	92632.190923	35.528640
1291.126134	92783.391178	35.533658
1292.353025	92893.083076	35.538676
1294.001325	93018.210713	35.543693
1294.828304	93134.342825	35.548711
1296.472110	93248.403953	35.553728
1297.665156	93361.247037	35.558746
1298.582596	93468.916407	35.563764
1300.227598	93563.934493	35.568781
1301.338238	93704.647739	35.573799
1302.802551	93776.798836	35.578816
1304.105947	93928.988150	35.583834
1305.003628	94017.219968	35.588852
1306.281049	94156.878574	35.593869
1307.806866	94265.119244	35.598887
1309.068517	94392.245297	35.603904
1310.139227	94481.697526	35.608922
1311.321964	94637.560546	35.613940
1313.001793	94728.896764	35.618957
1313.995469	94888.757573	35.623975
1315.289495	94986.709265	35.628992
1316.764418	95098.048873	35.634010
1317.845765	95278.430901	35.639028
1319.207083	95376.487465	35.644045
1320.335483	95523.939725	35.649063
1322.037041	95640.648035	35.654080
1323.283281	95782.693867	35.659098
1324.240250	95901.862376	35.664116
1325.733584	96038.632906	35.669133
1327.149338	96186.024864	35.674151
1328.504516	96317.650925	35.679168
1329.353798	96458.467342	35.684186
1330.890606	96590.053474	35.689204
1332.469664	96742.970896	35.694221
1333.547162	96879.945481	35.699239
1335.318503	97014.849560	35.704256
1336.493856	97138.380124	35.709274
1337.706715	97307.117663	35.714292
1339.359699	97419.262862	35.719309
1340.539499	97580.631480	35.724327
1342.238468	97715.285545	35.729344
1343.375219	97845.468580	35.734362
1344.595089	98017.911124	35.739380
1345.934326	98113.389351	35.744397
1347.130458	98289.684107	35.749415
1348.987294	98413.448595	35.754432
1350.373086	98548.524308	35.759450
1351.458311	98701.242421	35.764468
1353.207118	98840.380680	35.769485
1354.275068	98975.408216	35.774503
1355.881037	99109.035114	35.779520
1357.352429	99227.076490	35.784538
1358.677255	99400.253015	35.789556
1360.449110	99503.386803	35.794573
1361.543779	99659.867855	35.799591
1363.148968	99777.504876	35.804608
1364.516467	99915.805560	35.809626
1365.882585	100058.694237	35.814644
1367.363236	100156.701916	35.819661
1368.294324	100308.196198	35.824679
1369.623809	100415.744643	35.829696
1370.719509	100533.067914	35.834714
1372.197389	100671.849102	35.839732
1374.153407	100771.447847	35.844749
1374.895177	100890.126224	35.849767
1376.058899	101010.832410	35.854784
1377.378093	101155.747358	35.859802
1378.666561	101251.993342	35.864820
1380.529030	101409.370262	35.869837
1381.544434	101534.082550	35.874855
1382.791045	101649.900611	35.879872
1383.930527	101805.591859	35.884890
1385.078944	101923.641444	35.889908
1386.980945	102051.575416	35.894925
1387.777712	102202.711146	35.899943
1389.380514	102345.506737	35.904960
1390.891145	102499.333993	35.909978
1392.047330	102641.588613	35.914996
1393.362886	102776.814164	35.920013
1394.683625	102945.651871	35.925031
1396.540683	103086.234894	35.930048
1397.881678	103225.673209	35.935066
1399.012561	103363.684044	35.940084
1400.834551	103522.239648	35.945101
1401.957732	103690.519311	35.950119
1403.566461	103825.236069	35.955136
1404.984270	103973.361073	35.960154
1406.078025	104133.086961	35.965172
1407.784835	104268.980325	35.970189
1409.282422	104429.308480	35.975207
1410.737787	104595.485220	35.980224
1412.345880	104736.288546	35.985242
1413.913041	104866.759070	35.990260
1415.646852	105042.329929	35.995277
1416.819523	105164.296454	36.000295
1418.107340	105336.390250	36.005312
1419.875137	105451.277298	36.010330
1421.156447	105636.372581	36.015348
1422.683942	105751.634674	36.020365
1423.936173	105897.311002	36.025383
1425.568157	106040.535729	36.030400
1427.204702	106176.881549	36.035418
1428.707419	106350.834420	36.040436
1429.871192	106458.012942	36.045453
1431.307721	106629.592503	36.050471
1432.648391	106772.576805	36.055488
1434.465875	106883.646719	36.060506
1435.659170	107064.976211	36.065524
1437.080669	107189.514662	36.070541
1438.676819	107337.176645	36.075559
1439.890885	107493.285929	36.080576
1441.236872	107631.451956	36.085594
1442.698062	107776.391365	36.090612
1444.119097	107920.319072	36.095629
1445.322428	108066.788502	36.100647
1447.011377	108204.574215	36.105664
1448.203358	108342.294117	36.110682
1449.280145	108468.925590	36.115700
1450.924870	108590.878882	36.120717
1452.217123	108762.376338	36.125735
1453.440514	108875.480252	36.130752
1454.932220	109021.434957	36.135770
1456.164414	109187.457537	36.140788
1458.027115	109312.841935	36.145805
1459.297892	109474.910873	36.150823
1460.548834	109636.730868	36.155840
1462.148152	109770.773759	36.160858
1463.381237	109912.660799	36.165876
1465.255182	110084.296686	36.170893
1466.539870	110236.545115	36.175911
1467.889605	110383.093876	36.180928
1469.713738	110542.423566	36.185946
1471.186011	110718.742018	36.190964
1472.778394	110859.786260	36.195981
1474.058774	111011.875624	36.200999
1475.531674	111165.663367	36.206016
1477.186122	111318.594022	36.211034
1478.887155	111475.866832	36.216052
1480.134060	111632.351939	36.221069
1481.965482	111788.340051	36.226087
1483.357314	111931.403575	36.231104
1484.943734	112095.338684	36.236122
1486.362770	112266.562042	36.241140
1487.879959	112406.702909	36.246157
1489.645648	112570.846900	36.251175
1490.573670	112714.216531	36.256192
1492.499130	112870.329464	36.261210
1493.960772	113039.652332	36.266228
1495.406173	113202.040938	36.271245
1496.978310	113351.332009	36.276263
1498.231440	113487.526498	36.281280
1499.941764	113678.831207	36.286298
1501.097388	113833.426592	36.291316
1503.252291	113969.011982	36.296333
1504.466280	114167.704671	36.301351
1506.094327	114306.129379	36.306368
1507.703780	114462.853256	36.311386
1509.027667	114639.970189	36.316404
1510.925652	114783.666065	36.321421
1512.237200	114934.337435	36.326439
1513.594688	115113.864375	36.331456
1515.517887	115262.800864	36.336474
1516.850003	115411.483948	36.341492
1518.372952	115563.898133	36.346509
1520.253963	115742.814582	36.351527
1521.731951	115880.448777	36.356544
1522.953994	116033.173168	36.361562
1524.306258	116201.604096	36.366580
1525.833688	116353.560161	36.371597
1527.628687	116511.273932	36.376615
1529.237568	116638.951597	36.381632
1531.096897	116788.432706	36.386650
1531.984623	116935.144026	36.391668
1533.797860	117063.500454	36.396685
1534.917118	117203.098189	36.401703
1535.983407	117344.946391	36.406720
1537.591195	117486.829650	36.411738
1539.206432	117640.989096	36.416756
1540.436744	117790.740627	36.421773
1542.282745	117948.284239	36.426791
1543.587868	118107.345668	36.431808
1545.008382	118259.412381	36.436826
1546.403935	118425.793354	36.441844
1547.952968	118576.397922	36.446861
1549.694929	118754.268552	36.451879
1550.952597	118920.946891	36.456896
1552.908050	119084.438223	36.461914
1553.925612	119250.194404	36.466932
1555.735386	119420.201094	36.471949
1557.119853	119599.850266	36.476967
1558.993207	119759.680088	36.481984
1560.644662	119920.704895	36.487002
1562.255196	120092.976499	36.492020
1563.787718	120275.715840	36.497037
1565.959352	120443.943108	36.502055
1567.379829	120610.707757	36.507072
1569.257842	120751.945495	36.512090
1570.555614	120944.883604	36.517108
1572.285459	121097.620710	36.522125
1573.723294	121258.016497	36.527143
1575.140564	121437.210868	36.532160
1576.920016	121597.883749	36.537178
1578.413298	121760.452134	36.542196
1579.832476	121957.279165	36.547213
1581.739770	122111.425121	36.552231
1583.103200	122276.942933	36.557248
1585.007763	122459.461096	36.562266
1586.593647	122616.295410	36.567284
1588.127511	122788.793223	36.572301
1590.011386	122958.792144	36.577319
1591.311230	123134.065101	36.582336
1593.509383	123283.903439	36.587354
1594.886116	123457.342481	36.592372
1596.481029	123619.893496	36.597389
1598.579545	123803.745342	36.602407
1599.527687	123956.331850	36.607424
1601.502448	124089.250641	36.612442
1603.160497	124293.808618	36.617460
1604.633713	124437.701585	36.622477
1606.382951	124610.101001	36.627495
1608.105068	124772.208180	36.632512
1609.732749	124918.827772	36.637530
1611.244565	125101.008450	36.642548
1612.724878	125251.643183	36.647565
1614.263550	125401.243500	36.652583
1615.840657	125560.173834	36.657600
1617.296558	125719.998358	36.662618
1619.006642	125825.595111	36.667636
1620.650908	126006.164865	36.672653
1622.026023	126137.909704	36.677671
1623.432614	126289.524626	36.682688
1625.163588	126426.179793	36.687706
1626.646819	126604.866398	36.692724
1627.862692	126736.322762	36.697741
1629.569551	126918.902733	36.702759
1631.224941	127059.905295	36.707776
1632.786508	127225.979569	36.712794
1634.053266	127421.097518	36.717812
1635.787427	127560.582729	36.722829
1637.206635	127765.825629	36.727847
1638.966269	127918.837663	36.732864
1640.698180	128115.748840	36.737882
1642.271372	128278.027317	36.742900
1644.244804	128433.807870	36.747917
1645.869639	128652.389427	36.752935
1647.330635	128820.528895	36.757952
1649.375093	128998.964647	36.762970
1650.927168	129185.967508	36.767988
1652.465391	129337.591085	36.773005
1654.511880	129527.950861	36.778023
1655.818817	129706.546321	36.783040
1657.690556	129897.113746	36.788058
1659.600361	130062.275701	36.793076
1661.284560	130238.331602	36.798093
1662.810717	130423.307249	36.803111
1664.738583	130605.851234	36.808128
1666.244729	130779.683761	36.813146
1667.829727	130958.040383	36.818164
1669.870218	131123.162533	36.823181
1671.708959	131309.500682	36.828199
1673.170103	131494.620433	36.833216
1675.088725	131659.182307	36.838234
1676.980378	131841.714764	36.843252
1678.290274	132008.757220	36.848269
1680.206463	132185.802088	36.853287
1681.820897	132371.904166	36.858304
1683.511962	132539.877472	36.863322
1685.749518	132703.127814	36.868340
1686.925662	132898.767362	36.873357
1688.743964	133042.067700	36.878375
1690.275643	133248.954868	36.883392
1692.215252	133401.334904	36.888410
1694.223785	133568.364304	36.893428
1695.669495	133764.879260	36.898445
1697.581051	133923.931154	36.903463
1699.032440	134089.582313	36.908480
1700.726037	134268.956209	36.913498
1702.661277	134430.680654	36.918516
1704.213318	134613.183492	36.923533
1706.070277	134765.254494	36.928551
1707.579566	134925.174090	36.933568
1709.430651	135067.617773	36.938586
1711.032689	135222.240517	36.943604
1712.226720	135380.616159	36.948621
1713.991901	135529.930814	36.953639
1715.457458	135697.971165	36.958656
1716.650474	135852.370796	36.963674
1718.579286	136018.007929	36.968692
1720.292126	136190.953696	36.973709
1722.224544	136355.553129	36.978727
1723.418889	136534.703604	36.983744
1724.961527	136707.666799	36.988762
1727.116853	136892.445148	36.993780
1728.319091	137069.012621	36.998797
1730.302229	137243.150880	37.003815
1731.838353	137435.418688	37.008832
1733.892690	137615.871167	37.013850
1735.735506	137812.984157	37.018868
1737.185319	137997.830822	37.023885
1739.341188	138179.626569	37.028903
1740.780573	138377.238255	37.033920
1743.035299	138563.151861	37.038938
1744.704667	138734.877658	37.043956
1746.156695	138922.112193	37.048973
1748.191466	139107.760007	37.053991
1750.185398	139303.236853	37.059008
1751.659778	139482.753670	37.064026
1753.394933	139661.659883	37.069044
1755.044513	139882.186194	37.074061
1757.022339	140038.346128	37.079079
1758.796349	140244.712219	37.084096
1760.849077	140453.088546	37.089114
1762.979583	140624.308463	37.094132
1764.533852	140805.214606	37.099149
1766.430313	140981.289611	37.104167
1768.466435	141177.177568	37.109184
1770.128925	141358.602146	37.114202
1771.969141	141543.725665	37.119220
1773.528894	141712.773806	37.124237
1775.106686	141923.377586	37.129255
1777.057291	142095.825775	37.134272
1778.893491	142297.734833	37.139290
1780.874466	142479.470436	37.144308
1782.621517	142660.826018	37.149325
1784.877606	142845.815414	37.154343
1786.546158	143007.844635	37.159360
1788.234448	143216.310537	37.164378
1790.431478	143381.122247	37.169396
1792.054620	143556.850012	37.174413
1794.088572	143733.704976	37.179431
1795.639602	143916.391936	37.184448
1797.328828	144079.576939	37.189466
1799.346212	144286.007922	37.194484
1800.919157	144439.314246	37.199501
1802.669941	144622.886273	37.204519
1804.252733	144786.155287	37.209536
1806.227413	144927.777244	37.214554
1807.634428	145101.177881	37.219572
1809.430034	145267.242207	37.224589
1811.151084	145424.687375	37.229607
1812.418860	145612.436062	37.234624
1814.042048	145774.258865	37.239642
1816.273884	145950.309211	37.244660
1817.785397	146129.998718	37.249677
1819.657001	146304.004098	37.254695
1821.771161	146487.846333	37.259712
1823.165003	146667.823794	37.264730
1825.272515	146855.002973	37.269748
1826.454179	147054.296347	37.274765
1828.516028	147234.411846	37.279783
1830.289631	147429.924898	37.284800
1832.237439	147616.601556	37.289818
1834.200224	147803.593843	37.294836
1835.986005	147997.536613	37.299853
1838.151373	148199.786744	37.304871
1839.844298	148391.756463	37.309888
1841.579648	148575.341392	37.314906
1843.758635	148784.413069	37.319924
1845.456606	148983.750683	37.324941
1847.600654	149170.139095	37.329959
1849.149557	149363.899593	37.334976
1851.309190	149558.426346	37.339994
1853.274607	149749.955296	37.345012
1855.164878	149952.348919	37.350029
1857.099550	150143.378004	37.355047
1858.889667	150332.491546	37.360064
1860.744504	150526.007632	37.365082
1862.716736	150722.954495	37.370100
1864.571748	150929.327858	37.375117
1866.658992	151118.474886	37.380135
1868.647104	151296.469753	37.385152
1870.176361	151509.224640	37.390170
1872.314868	151675.470817	37.395188
1874.367382	151880.804632	37.400205
1876.236998	152087.664763	37.405223
1878.403665	152271.620587	37.410240
1880.262893	152440.298445	37.415258
1882.222991	152655.477286	37.420276
1884.265507	152829.643046	37.425293
1886.412203	153011.159278	37.430311
1887.840034	153217.120398	37.435328
1889.891779	153394.203696	37.440346
1891.598780	153573.992467	37.445364
1893.426884	153786.397665	37.450381
1895.202942	153973.391754	37.455399
1896.931675	154156.375246	37.460416
1899.024458	154358.434273	37.465434
1901.202647	154528.010363	37.470452
1902.816212	154740.937484	37.475469
1905.126190	154917.087684	37.480487
1907.035957	155070.644814	37.485504
1908.515164	155256.881730	37.490522
1910.107242	155411.847509	37.495540
1912.225485	155564.486262	37.500557
1914.137819	155764.617107	37.505575
1915.837337	155918.984914	37.510592
1917.309495	156098.672344	37.515610
1919.393355	156253.284982	37.520628
1920.995470	156476.469920	37.525645
1923.007204	156648.542940	37.530663
1924.749191	156823.208268	37.535680
1926.764911	157041.500286	37.540698
1928.766760	157220.615057	37.545716
1930.220907	157393.667918	37.550733
1932.304763	157624.379183	37.555751
1934.223919	157807.808675	37.560768
1935.866697	158010.049650	37.565786
1938.193651	158206.109394	37.570804
1940.308841	158423.709676	37.575821
1942.520210	158610.546109	37.580839
1944.536199	158804.642420	37.585856
1946.453817	159013.046386	37.590874
1948.541057	159214.196736	37.595892
1950.479782	159406.241729	37.600909
1952.081353	159598.569538	37.605927
1954.082345	159799.470655	37.610944
1956.437288	160018.234859	37.615962
1958.779551	160203.473953	37.620980
1960.553951	160410.539438	37.625997
1962.424352	160622.523859	37.631015
1964.898878	160814.402770	37.636032
1966.714680	161017.889157	37.641050
1968.782191	161203.468782	37.646068
1970.962176	161412.517472	37.651085
1973.148185	161599.449957	37.656103
1975.534302	161795.748686	37.661120
1977.107868	161966.383068	37.666138
1979.190935	162172.141707	37.671156
1980.983976	162357.618730	37.676173
1983.042173	162554.557030	37.681191
1985.623129	162736.765899	37.686208
1987.223500	162938.433202	37.691226
1989.134300	163137.655475	37.696244
1991.362350	163313.556902	37.701261
1992.971816	163524.547362	37.706279
1995.565357	163709.118036	37.711296
1997.044407	163887.880468	37.716314
1999.276132	164098.192143	37.721332
2000.964609	164288.426200	37.726349
2003.035867	164459.234378	37.731367
2005.197832	164655.470122	37.736384
2006.628699	164881.931444	37.741402
2008.856883	165037.587070	37.746420
2010.970166	165228.811278	37.751437
2013.288208	165441.082812	37.756455
2015.212941	165612.959613	37.761472
2017.350212	165777.942030	37.766490
2018.764481	165953.325803	37.771508
2020.482291	166112.567466	37.776525
2022.262982	166296.519192	37.781543
2024.324526	166503.079402	37.786560
2025.950734	166679.409585	37.791578
2028.394335	166825.538839	37.796596
2030.428623	167014.501826	37.801613
2032.332039	167255.742212	37.806631
2034.434025	167433.598581	37.811648
2035.899768	167615.818415	37.816666
2037.923784	167802.503971	37.821684
2040.591303	167996.330731	37.826701
2042.678879	168189.388012	37.831719
2044.949502	168419.060767	37.836736
2046.639911	168587.411611	37.841754
2048.768370	168820.622791	37.846772
2050.556375	168989.746340	37.851789
2052.909294	169206.840960	37.856807
2054.916558	169380.776780	37.861824
2056.751076	169615.701086	37.866842
2059.001777	169805.074959	37.871860
2061.246068	170042.765466	37.876877
2063.018429	170224.048574	37.881895
2065.833149	170431.259137	37.886912
2067.634895	170625.312749	37.891930
2069.737144	170852.147446	37.896948
2072.226510	171036.504458	37.901965
2074.119845	171262.283818	37.906983
2076.906494	171426.591670	37.912000
2078.745494	171672.626990	37.917018
2081.018463	171827.605845	37.922036
2083.491049	172048.287312	37.927053
2085.169827	172220.118891	37.932071
2087.543194	172440.158683	37.937088
2089.803138	172623.811176	37.942106
2091.729302	172825.746191	37.947124
2093.906682	173033.249300	37.952141
2095.825164	173223.910317	37.957159
2098.253686	173411.675169	37.962176
2100.263688	173618.611683	37.967194
2102.926585	173790.306662	37.972212
2104.776279	173998.336170	37.977229
2107.035529	174167.331342	37.982247
2109.059758	174347.324993	37.987264
2111.056227	174543.307970	37.992282
2113.445188	174734.853017	37.997300
2115.222247	174921.941799	38.002317
2117.160440	175113.078089	38.007335
2119.656797	175286.987899	38.012352
2121.727229	175492.440235	38.017370
2123.696785	175676.634918	38.022388
2126.079261	175854.726296	38.027405
2127.734974	176051.163918	38.032423
2130.034326	176194.217801	38.037440
2131.704813	176372.081855	38.042458
2133.939831	176554.246639	38.047476
2136.018649	176709.402112	38.052493
2138.007241	176872.552313	38.057511
2140.183224	177051.645847	38.062528
2142.148611	177218.327974	38.067546
2143.924450	177392.944649	38.072564
2146.217147	177576.995137	38.077581
2148.128199	177748.382121	38.082599
2150.630077	177934.113736	38.087616
2152.342492	178121.024422	38.092634
2154.383708	178318.667719	38.097652
2156.480174	178514.768058	38.102669
2158.561651	178700.036920	38.107687
2161.153451	178901.008469	38.112704
2162.865633	179097.819539	38.117722
2165.053415	179298.248087	38.122740
2167.590248	179503.684471	38.127757
2169.497248	179707.204459	38.132775
2171.818423	179910.393298	38.137792
2174.150799	180121.561780	38.142810
2176.122820	180311.333780	38.147828
2178.469078	180537.676465	38.152845
2180.530412	180719.785474	38.157863
2182.894703	180916.438118	38.162880
2184.932146	181134.852351	38.167898
2187.444805	181338.931150	38.172916
2189.350695	181549.565314	38.177933
2191.670772	181765.539901	38.182951
2194.061043	181976.035880	38.187968
2196.544944	182186.619538	38.192986
2199.124829	182386.886191	38.198004
2201.390919	182579.755538	38.203021
2203.717038	182796.241828	38.208039
2206.033448	182986.427762	38.213056
2208.343009	183190.788565	38.218074
2210.240529	183387.818290	38.223092
2212.684829	183585.434671	38.228109
2214.805089	183778.675016	38.233127
2217.297874	183973.290942	38.238144
2219.179577	184180.173097	38.243162
2221.543029	184381.663226	38.248180
2223.685331	184584.052181	38.253197
2225.607117	184796.323590	38.258215
2228.283635	184991.105170	38.263232
2230.428889	185189.816613	38.268250
2232.582342	185419.108232	38.273268
2234.827068	185600.421725	38.278285
2237.126374	185796.205614	38.283303
2239.713745	186001.296619	38.288320
2241.954967	186211.138477	38.293338
2244.309867	186392.602638	38.298356
2246.789137	186591.749478	38.303373
2248.480531	186781.974568	38.308391
2250.778557	186954.542011	38.313408
2252.792442	187147.420339	38.318426
2254.915179	187315.499469	38.323444
2256.821686	187475.682491	38.328461
2258.770752	187658.586516	38.333479
2261.266973	187853.637392	38.338496
2263.201228	188037.293959	38.343514
2265.329287	188221.846879	38.348532
2267.249477	188413.831693	38.353549
2269.161006	188624.587080	38.358567
2271.385037	188833.859896	38.363584
2273.664364	189053.429198	38.368602
2275.883915	189241.588310	38.373620
2278.075257	189479.396545	38.378637
2280.399740	189674.317297	38.383655
2282.525437	189912.696494	38.388672
2285.297528	190130.086093	38.393690
2287.351415	190347.869760	38.398708
2290.100406	190566.166037	38.403725
2291.708429	190798.895676	38.408743
2294.607547	191016.548372	38.413760
2296.602048	191247.315321	38.418778
2299.002127	191467.079690	38.423796
2301.730278	191691.171350	38.428813
2303.685553	191923.622932	38.433831
2306.126520	192143.295056	38.438848
2308.397079	192372.729133	38.443866
2311.167282	192612.504368	38.448884
2313.650511	192828.149835	38.453901
2315.970822	193058.391469	38.458919
2318.228307	193290.458978	38.463936
2320.564107	193514.798899	38.468954
2322.848365	193740.683656	38.473972
2325.303945	193967.417980	38.478989
2328.081608	194193.328098	38.484007
2330.673745	194414.509362	38.489024
2332.803867	194641.856781	38.494042
2335.204953	194874.200821	38.499060
2337.946211	195083.329793	38.504077
2339.692190	195305.448712	38.509095
2342.282611	195533.945582	38.514112
2344.607086	195759.287316	38.519130
2346.516815	195992.602824	38.524148
2349.055727	196207.771763	38.529165
2350.665016	196447.838304	38.534183
2353.203229	196685.372596	38.539200
2356.051897	196909.900159	38.544218
2358.502845	197147.729646	38.549236
2360.527298	197377.009845	38.554253
2362.880763	197616.253077	38.559271
2365.277579	197834.116703	38.564288
2367.923943	198073.340983	38.569306
2370.049910	198327.867063	38.574324
2372.500145	198548.492140	38.579341
2374.798209	198774.181198	38.584359
2376.945062	198986.022206	38.589376
2379.022092	199222.701910	38.594394
2381.181444	199431.915342	38.599412
2383.959132	199630.318909	38.604429
2385.837153	199851.509751	38.609447
2387.721370	200077.688806	38.614464
2390.276180	200314.868781	38.619482
2392.598180	200539.051055	38.624500
2394.802126	200768.292091	38.629517
2397.016588	201023.413560	38.634535
2399.585570	201249.996685	38.639552
2401.800391	201492.858754	38.644570
2403.892597	201747.050994	38.649588
2406.784949	201988.728931	38.654605
2408.655096	202242.933273	38.659623
2411.153083	202499.527162	38.664640
2413.867116	202753.587380	38.669658
2415.878795	203024.756702	38.674676
2418.742399	203282.349800	38.679693
2421.060414	203540.157501	38.684711
2423.610807	203806.853208	38.689728
2426.341780	204068.685232	38.694746
2428.710460	204322.248755	38.699764
2431.341514	204575.429083	38.704781
2433.705298	204840.915222	38.709799
2436.062366	205124.124446	38.714816
2439.191633	205358.289844	38.719834
2441.377591	205635.334012	38.724852
2443.828791	205896.457075	38.729869
2446.575395	206161.444302	38.734887
2448.875101	206410.978482	38.739904
2451.502788	206671.759678	38.744922
2453.824984	206949.702465	38.749940
2456.565844	207203.765444	38.754957
2459.066136	207478.864321	38.759975
2461.571658	207721.795664	38.764992
2463.929714	207998.061985	38.770010
2466.655064	208274.080941	38.775028
2469.101364	208532.766326	38.780045
2471.822540	208772.874898	38.785063
2474.063384	209043.693134	38.790080
2476.823701	209300.732472	38.795098
2479.021387	209560.375657	38.800116
2481.844781	209819.286020	38.805133
2484.144628	210078.927892	38.810151
2486.506774	210353.376142	38.815168
2489.336070	210607.959841	38.820186
2492.033429	210877.317300	38.825204
2494.287147	211125.430912	38.830221
2496.470585	211368.453131	38.835239
2498.878729	211667.731830	38.840256
2501.680812	211907.827011	38.845274
2503.787505	212183.745600	38.850292
2506.637398	212451.981073	38.855309
2508.579002	212721.808904	38.860327
2511.226715	212955.978257	38.865344
2514.073673	213192.110098	38.870362
2516.200173	213430.223240	38.875380
2518.587272	213665.896456	38.880397
2521.118856	213912.897657	38.885415
2523.513157	214145.905339	38.890432
2525.692346	214396.125457	38.895450
2527.780826	214651.591617	38.900468
2530.484950	214902.568385	38.905485
2532.693785	215169.812017	38.910503
2535.213254	215438.708760	38.915520
2537.747798	215707.299478	38.920538
2539.829890	215973.995051	38.925556
2542.684076	216241.927812	38.930573
2545.407413	216524.787790	38.935591
2548.004772	216798.959212	38.940608
2550.772475	217088.391173	38.945626
2553.340905	217376.611667	38.950644
2555.819794	217641.473309	38.955661
2558.559820	217918.813354	38.960679
2560.841563	218197.382500	38.965696
2563.572434	218484.388318	38.970714
2565.758480	218769.564427	38.975732
2568.683158	219065.099439	38.980749
2571.045609	219360.191489	38.985767
2573.808485	219649.583898	38.990784
2576.636954	219938.903584	38.995802
2579.091439	220240.802858	39.000820
2581.920130	220516.234338	39.005837
2584.707402	220811.455396	39.010855
2587.360000	221096.757147	39.015872
2590.091570	221443.476252	39.020890
2592.672655	221748.053393	39.025908
2595.280255	222034.381616	39.030925
2598.331650	222323.687955	39.035943
2600.705410	222606.855667	39.040960
2603.554810	222890.329984	39.045978
2605.973996	223194.075130	39.050996
2608.904633	223468.866349	39.056013
2611.581108	223764.319595	39.061031
2614.080489	224057.275195	39.066048
2616.760935	224331.271040	39.071066
2619.621900	224620.857362	39.076084
2621.846915	224906.520318	39.081101
2624.758166	225204.989190	39.086119
2627.173685	225487.436890	39.091136
2630.014677	225775.176658	39.096154
2632.482015	226080.398150	39.101172
2635.242557	226353.486631	39.106189
2638.160410	226653.648587	39.111207
2640.462306	226946.937995	39.116224
2643.153272	227220.814934	39.121242
2645.984664	227527.380858	39.126260
2648.460601	227802.563567	39.131277
2651.616472	228082.210800	39.136295
2653.977593	228345.451749	39.141312
2656.753191	228592.678811	39.146330
2658.665872	228852.411439	39.151348
2661.433038	229098.828590	39.156365
2663.792178	229359.101520	39.161383
2665.771716	229631.346478	39.166400
2668.470626	229902.106879	39.171418
2671.016689	230181.603490	39.176436
2673.538436	230469.917615	39.181453
2676.110127	230755.075502	39.186471
2678.675751	231046.381382	39.191488
2681.429776	231336.464673	39.196506
2683.798207	231645.048481	39.201524
2686.698241	231932.037433	39.206541
2689.364599	232230.924951	39.211559
2691.897868	232539.180841	39.216576
2694.901041	232840.683698	39.221594
2697.446984	233153.638161	39.226612
2700.127781	233464.718239	39.231629
2702.884761	233781.628788	39.236647
2705.474536	234095.874662	39.241664
2708.607069	234414.861218	39.246682
2711.209904	234733.856516	39.251700
2713.658982	235043.530615	39.256717
2716.752008	235367.707742	39.261735
2719.178276	235690.239028	39.266752
2722.316447	236014.309479	39.271770
2725.043817	236337.455476	39.276788
2727.555227	236661.170061	39.281805
2730.245986	236995.600928	39.286823
2733.067765	237324.652944	39.291840
2736.262207	237648.948150	39.296858
2739.086015	237982.624484	39.301876
2741.939320	238307.940874	39.306893
2744.773244	238620.231532	39.311911
2747.488460	238956.899752	39.316928
2750.415049	239280.810457	39.321946
2752.957971	239618.777932	39.326964
2756.066533	239924.602704	39.331981
2758.642723	240264.827388	39.336999
2761.371639	240594.310252	39.342016
2764.275930	240908.120073	39.347034
2767.019796	241242.631538	39.352052
2769.813910	241574.215012	39.357069
2772.807221	241909.044445	39.362087
2775.288525	242233.567313	39.367104
2778.180175	242560.134260	39.372122
2780.975133	242898.934833	39.377140
2783.711488	243228.499952	39.382157
2786.533246	243558.128612	39.387175
2789.248221	243895.268127	39.392192
2792.354702	244223.075395	39.397210
2794.733710	244556.917001	39.402228
2797.554223	244893.178786	39.407245
2800.513994	245207.930506	39.412263
2803.089542	245516.749273	39.417280
2805.488251	245809.797538	39.422298
2808.140588	246125.565311	39.427316
2811.017230	246426.616638	39.432333
2814.051144	246727.643712	39.437351
2816.183164	247058.126876	39.442368
2818.902514	247355.217160	39.447386
2821.383140	247685.265553	39.452404
2824.586467	248013.803192	39.457421
2827.411858	248337.422795	39.462439
2829.636658	248672.721139	39.467456
2832.691293	249003.037188	39.472474
2835.297320	249345.439794	39.477492
2838.204011	249690.665897	39.482509
2841.064523	250031.556436	39.487527
2843.347402	250385.519312	39.492544
2846.635760	250745.496314	39.497562
2848.997879	251095.231541	39.502580
2852.022211	251452.152908	39.507597
2854.978959	251812.159335	39.512615
2858.098106	252180.091544	39.517632
2861.005732	252547.829411	39.522650
2864.155746	252917.993643	39.527668
2866.984024	253279.217322	39.532685
2870.093028	253645.452251	39.537703
2873.111978	254007.536241	39.542720
2876.568047	254359.721136	39.547738
2879.580007	254730.749127	39.552756
2882.231836	255087.152424	39.557773
2885.584992	255437.399607	39.562791
2888.265808	255805.738613	39.567808
2891.039350	256160.016155	39.572826
2893.836664	256524.654669	39.577844
2896.729052	256887.322776	39.582861
2899.968471	257243.458940	39.587879
2902.693457	257623.529994	39.592896
2905.899982	257970.934097	39.597914
2908.964721	258342.493543	39.602932
2911.718948	258712.959624	39.607949
2914.891600	259057.601822	39.612967
2917.497412	259443.562681	39.617984
2920.644590	259796.364178	39.623002
2923.425655	260167.844288	39.628020
2926.438467	260529.254161	39.633037
2929.651125	260892.665101	39.638055
2932.125029	261266.227576	39.643072
2935.285271	261632.315071	39.648090
2938.297423	262007.038038	39.653108
2940.964776	262376.202026	39.658125
2944.259773	262741.177228	39.663143
2946.633790	263108.838947	39.668160
2949.890846	263479.587467	39.673178
2953.067872	263848.443844	39.678196
2955.878768	264223.988765	39.683213
2958.952150	264577.391882	39.688231
2961.568407	264918.877455	39.693248
2964.550164	265261.118377	39.698266
2967.118155	265582.035679	39.703284
2969.871524	265937.573761	39.708301
2973.050244	266258.928381	39.713319
2975.450314	266616.733032	39.718336
2978.331323	266961.277581	39.723354
2981.249229	267309.474605	39.728372
2983.829483	267679.292667	39.733389
2986.982598	268026.817882	39.738407
2989.414756	268425.289370	39.743424
2992.480210	268784.412830	39.748442
2995.438712	269164.231719	39.753460
2997.805016	269555.067999	39.758477
3001.301340	269928.324364	39.763495
3004.065840	270326.337999	39.768512
3007.063015	270728.100112	39.773530
3010.248097	271115.073327	39.778548
3013.174815	271531.784144	39.783565
3016.799334	271921.787350	39.788583
3019.491425	272334.242457	39.793600
3022.831714	272728.812730	39.798618
3026.001614	273135.629122	39.803636
3029.274827	273540.676430	39.808653
3032.379291	273942.321074	39.813671
3035.458481	274341.048393	39.818688
3038.524653	274755.858190	39.823706
3041.584893	275162.235029	39.828724
3044.625312	275569.326322	39.833741
3048.128474	275969.841106	39.838759
3051.134186	276385.295611	39.843776
3053.746237	276791.768772	39.848794
3057.411150	277199.955109	39.853812
3060.428012	277608.243949	39.858829
3063.949423	278014.954057	39.863847
3066.958775	278429.848795	39.868864
3070.303375	278826.653954	39.873882
3073.396762	279230.941940	39.878900
3076.295274	279635.616271	39.883917
3079.429696	280026.179648	39.888935
3082.793224	280450.543865	39.893952
3085.243871	280849.521988	39.898970
3088.620404	281253.789695	39.903988
3091.383645	281666.638938	39.909005
3094.520485	282077.904611	39.914023
3097.797931	282502.382873	39.919040
3100.870490	282899.152903	39.924058
3104.070932	283326.538720	39.929076
3106.888482	283739.682776	39.934093
3110.233513	284146.188999	39.939111
3113.578535	284565.371064	39.944128
3116.582967	284985.749784	39.949146
3119.840094	285404.284492	39.954164
3123.267984	285811.690608	39.959181
3126.230846	286203.928056	39.964199
3128.924601	286582.337627	39.969216
3132.095413	286961.077775	39.974234
3135.017336	287331.067475	39.979252
3137.585876	287713.382333	39.984269
3140.846755	288090.074772	39.989287
3143.332150	288490.768216	39.994304
3146.081753	288891.012904	39.999322
3149.483943	289285.158744	40.004340
3152.146343	289709.320222	40.009357
3155.175786	290105.098921	40.014375
3158.330915	290524.253092	40.019392
3161.355763	290947.898111	40.024410
3164.568620	291370.064759	40.029428
3167.436678	291809.635256	40.034445
3170.973240	292244.221925	40.039463
3174.387454	292681.316631	40.044480
3177.203354	293125.668701	40.049498
3180.551893	293560.358942	40.054516
3183.753749	294008.077574	40.059533
3186.592284	294458.570836	40.064551
3189.979382	294909.179590	40.069568
3193.375454	295350.717379	40.074586
3196.783691	295804.673955	40.079604
3199.569511	296274.680501	40.084621
3203.411640	296724.070178	40.089639
3206.543204	297191.403414	40.094656
3209.674647	297647.126845	40.099674
3213.418431	298099.907274	40.104692
3216.485777	298564.605420	40.109709
3220.281874	299009.272120	40.114727
3223.207239	299479.934318	40.119744
3226.589667	299931.573338	40.124762
3229.819293	300390.398544	40.129780
3233.178262	300851.513543	40.134797
3236.392742	301308.458861	40.139815
3239.737301	301771.605606	40.144832
3242.632119	302244.093566	40.149850
3246.265812	302688.928356	40.154868
3249.628001	303168.401028	40.159885
3253.213343	303629.725955	40.164903
3256.408049	304103.608457	40.169920
3259.508622	304550.909635	40.174938
3263.255975	305006.133715	40.179956
3265.926839	305478.214813	40.184973
3269.889618	305942.241151	40.189991
3273.345536	306407.971697	40.195008
3276.476140	306853.050757	40.200026
3280.177815	307302.965629	40.205044
3282.884027	307766.574698	40.210061
3286.038684	308220.103500	40.215079
3289.453202	308680.853960	40.220096
3292.724163	309148.483387	40.225114
3296.348064	309605.285670	40.230132
3299.649382	310072.982922	40.235149
3302.829678	310502.725029	40.240167
3305.779042	310936.185018	40.245184
3308.834451	311353.370966	40.250202
3312.007423	311762.561401	40.255220
3315.191054	312180.816203	40.260237
3318.373830	312616.798187	40.265255
3321.439804	313041.646737	40.270272
3324.648964	313471.144395	40.275290
3328.032485	313917.680795	40.280308
3330.808875	314359.358594	40.285325
3334.253920	314808.929359	40.290343
3337.444577	315258.792402	40.295360
3339.994335	315723.511321	40.300378
3343.573412	316184.992132	40.305396
3346.657156	316667.299475	40.310413
3350.156802	317144.611481	40.315431
3353.351056	317636.700265	40.320448
3356.793655	318127.299605	40.325466
3360.309544	318604.271700	40.330484
3363.365921	319107.956084	40.335501
3366.484762	319601.214953	40.340519
3370.158670	320102.154981	40.345536
3373.685967	320601.947193	40.350554
3377.283455	321102.868415	40.355572
3380.494683	321612.965388	40.360589
3384.325329	322121.844019	40.365607
3387.540266	322630.359930	40.370624
3390.902472	323146.874830	40.375642
3394.847396	323643.155261	40.380660
3397.857682	324162.081523	40.385677
3401.659128	324677.070085	40.390695
3405.240063	325181.043169	40.395712
3408.777230	325688.702452	40.400730
3412.515765	326197.164781	40.405748
3416.278665	326712.197434	40.410765
3419.857614	327218.545323	40.415783
3423.405122	327719.942923	40.420800
3426.436669	328225.278907	40.425818
3430.161086	328730.171911	40.430836
3433.814997	329233.422105	40.435853
3437.182808	329735.774618	40.440871
3440.947102	330238.492794	40.445888
3444.325402	330750.359654	40.450906
3448.028720	331254.096361	40.455924
3451.334220	331754.718307	40.460941
3454.736680	332247.982770	40.465959
3458.479590	332758.762161	40.470976
3461.724329	333257.021698	40.475994
3465.617875	333748.395242	40.481012
3468.822437	334253.789487	40.486029
3472.125448	334746.442836	40.491047
3475.907563	335255.750477	40.496064
3478.996001	335747.160955	40.501082
3482.797515	336253.766496	40.506100
3486.231280	336753.011962	40.511117
3489.653941	337245.393613	40.516122
3493.042785	337685.228990	40.521127
3495.491467	338101.103038	40.526132
3498.604868	338441.417598	40.531136
3500.955424	338760.493441	40.536141
3503.170231	339007.549161	40.541146
3505.425728	339226.392522	40.546151
3507.132267	339412.865931	40.551156
3508.956054	339555.256580	40.556160
3510.001661	339649.735250	40.561165
3511.267046	339729.949380	40.566170
3512.692915	339775.518510	40.571175
3513.267507	339803.886973	40.576180
3514.162949	339777.602590	40.581184
3514.737653	339760.456531	40.586189
3515.247250	339715.981491	40.591194
3515.723609	339648.168900	40.596199
3516.097609	339572.302987	40.601204
3516.151980	339480.577729	40.606208
3516.221293	339400.228672	40.611213
3516.364187	339282.091578	40.616218
3516.774072	339165.083024	40.621223
3516.554920	339059.450633	40.626228
3516.655878	338917.925591	40.631232
3516.542070	338814.567173	40.636237
3516.055766	338675.298192	40.641242
3515.853003	338546.726530	40.646247
3515.653050	338423.347209	40.651252
3515.360062	338285.345088	40.656256
3514.844353	338174.259609	40.661261
3514.901825	338032.484947	40.666266
3514.798811	337922.224765	40.671271
3514.672754	337805.934894	40.676276
3514.254697	337674.137139	40.681280
3513.786775	337563.093981	40.686285
3513.882059	337442.135407	40.691290
3513.683925	337323.564996	40.696295
3513.175874	337215.378726	40.701300
3513.108358	337109.286444	40.706304
3512.704868	336983.772785	40.711309
3512.250773	336885.174596	40.716314
3512.238895	336785.488083	40.721319
3511.513664	336695.842326	40.726324
3511.655052	336593.840189	40.731328
3511.237220	336504.552887	40.736333
3511.329525	336415.821240	40.741338
3511.220683	336337.074915	40.746343
3510.940949	336240.739331	40.751348
3510.892180	336156.637345	40.756352
3510.442172	336082.094140	40.761357
3510.222920	336001.201035	40.766362
3510.237712	335917.165073	40.771367
3509.991245	335854.834274	40.776372
3509.815287	335778.261758	40.781376
3509.681653	335701.809750	40.786381
3509.389721	335646.639397	40.791386
3509.241761	335578.666743	40.796391
3508.832526	335515.419449	40.801396
3508.932950	335457.844853	40.806400
3508.676011	335402.566941	40.811405
3508.872624	335352.308732	40.816410
3508.724393	335282.859305	40.821415
3508.478820	335236.184021	40.826420
3508.147884	335189.725859	40.831424
3508.267319	335136.730303	40.836429
3507.764834	335091.953921	40.841434
3508.129692	335036.831986	40.846439
3507.746745	334999.266538	40.851444
3508.078174	334946.924670	40.856448
3507.576632	334915.207670	40.861453
3507.756032	334857.645542	40.866458
3507.713724	334819.186047	40.871463
3507.531857	334788.105801	40.876468
3507.555514	334733.470341	40.881472
3507.344244	334712.297668	40.886477
3506.988623	334667.345047	40.891482
3507.135353	334632.826934	40.896487
3507.041603	334607.435159	40.901492
3507.026042	334570.651495	40.906496
3506.753806	334544.855136	40.911501
3506.771404	334503.178344	40.916506
3506.839745	334477.837268	40.921511
3506.559528	334449.649124	40.926516
3506.673019	334416.994562	40.931520
3506.812154	334391.464060	40.936525
3506.599680	334371.487981	40.941530
3506.724559	334327.248361	40.946535
3506.632794	334310.817249	40.951540
3506.753386	334278.110583	40.956544
3506.094659	334254.666407	40.961549
3506.128069	334230.603647	40.966554
3506.203730	334202.359140	40.971559
3506.297351	334179.025116	40.976564
3506.250327	334159.048276	40.981568
3506.084774	334142.934282	40.986573
3506.108998	334124.600919	40.991578
3506.401385	334092.987146	40.996583
3506.117549	334080.990529	41.001588
3506.302168	334055.198137	41.006592
3506.168873	334029.888776	41.011597
3506.129266	334010.012552	41.016602
3506.214492	333988.690953	41.021607
3505.912168	333968.805336	41.026612
3506.031544	333946.129064	41.031616
3506.084059	333932.169914	41.036621
3506.129091	333913.171304	41.041626
3506.074944	333898.948974	41.046631
3505.852228	333883.785896	41.051636
3506.134675	333851.486225	41.056640
3505.942946	333837.871163	41.061645
3505.673295	333818.871361	41.066650
3506.020093	333801.810723	41.071655
3505.687771	333776.990976	41.076660
3505.896143	333762.447080	41.081664
3505.799031	333752.228393	41.086669
3505.932544	333736.474351	41.091674
3506.181551	333701.303161	41.096679
3505.738403	333686.938624	41.101684
3506.028162	333664.973602	41.106688
3505.760946	333644.802306	41.111693
3505.624788	333637.059190	41.116698
3505.825695	333614.929995	41.121703
3505.476340	333593.244196	41.126708
3505.225313	333579.409338	41.131712
3504.982682	333575.527190	41.136717
3505.316234	333559.639651	41.141722
3505.375140	333544.813845	41.146727
3505.264640	333537.244866	41.151732
3505.528317	333523.303167	41.156736
3505.734280	333518.077201	41.161741
3505.535039	333508.918399	41.166746
3505.754117	333482.560274	41.171751
3505.878047	333469.989928	41.176756
3505.819324	333451.364008	41.181760
3505.926010	333440.985766	41.186765
3505.639688	333420.791969	41.191770
3505.856401	333402.427986	41.196775
3505.481651	333383.317392	41.201780
3505.509069	333372.111559	41.206784
3505.430994	333360.133206	41.211789
3505.337802	333345.866021	41.216794
3505.623344	333320.210151	41.221799
3505.676436	333314.193681	41.226804
3505.401732	333304.741288	41.231808
3505.178112	333283.391928	41.236813
3505.146005	333266.009193	41.241818
3505.610567	333259.469423	41.246823
3505.458197	333246.688139	41.251828
3505.727229	333227.781221	41.256832
3505.663911	333214.858563	41.261837
3505.740727	333205.019628	41.266842
3505.626878	333171.662144	41.271847
3505.300790	333161.963274	41.276852
3505.116556	333144.553644	41.281856
3505.335618	333147.192118	41.286861
3505.264609	333125.767668	41.291866
3505.629363	333121.178478	41.296871
3504.736378	333115.718889	41.301876
3505.092830	333104.180957	41.306880
3505.632172	333090.781128	41.311885
3505.247349	333076.229039	41.316890
3505.332213	333071.200391	41.321895
3505.268035	333055.171953	41.326900
3505.030513	333043.549709	41.331904
3505.110893	333035.237673	41.336909
3504.898037	333030.332464	41.341914
3505.152627	333015.042822	41.346919
3504.813217	333015.452905	41.351924
3505.304967	332999.209275	41.356928
3505.275118	332987.223234	41.361933
3505.258899	332978.519133	41.366938
3505.544566	332956.452707	41.371943
3505.008671	332952.871469	41.376948
3505.215283	332935.323623	41.381952
3504.897448	332942.094828	41.386957
3504.819587	332932.942221	41.391962
3505.359720	332908.264278	41.396967
3505.140589	332909.088135	41.401972
3505.057120	332888.276578	41.406976
3505.144344	332883.451209	41.411981
3505.131099	332875.281247	41.416986
3505.466593	332859.596909	41.421991
3504.984140	332856.923711	41.426996
3505.395824	332842.322026	41.432000
3505.303270	332829.607585	41.437005
3504.930061	332809.427349	41.442010
3505.131037	332806.086024	41.447015
3504.809795	332788.417926	41.452020
3505.039158	332789.934625	41.457024
3505.256951	332778.749519	41.462029
3505.105922	332776.533086	41.467034
3504.996713	332765.119634	41.472039
3504.940996	332752.017482	41.477044
3504.889685	332753.654929	41.482048
3504.969666	332745.317464	41.487053
3504.662352	332748.115546	41.492058
3505.145312	332728.181804	41.497063
3504.688742	332724.715306	41.502068
3505.389445	332703.015976	41.507072
3505.320119	332700.455667	41.512077
3505.216740	332685.248006	41.517082
3505.160595	332674.055274	41.522087
3504.822208	332665.987607	41.527092
3505.122326	332650.996189	41.532096
3505.311568	332654.097645	41.537101
3505.165094	332639.940575	41.542106
3505.156903	332622.222944	41.547111
3504.710551	332612.721220	41.552116
3504.845800	332605.673372	41.557120
3504.885385	332602.484844	41.562125
3504.828846	332588.109879	41.567130
3505.069648	332587.409906	41.572135
3504.760240	332587.713415	41.577140
3505.102072	332564.314159	41.582144
3505.166720	332560.943458	41.587149
3504.948485	332557.261064	41.592154
3505.238320	332523.839456	41.597159
3505.108390	332531.853908	41.602164
3504.808473	332510.847336	41.607168
3505.077458	332510.906655	41.612173
3504.662836	332518.202367	41.617178
3504.832948	332492.971781	41.622183
3504.591238	332493.366421	41.627188
3504.880105	332482.195490	41.632192
3505.168381	332479.476805	41.637197
3504.618830	332472.028041	41.642202
3505.235539	332469.257432	41.647207
3504.955221	332446.898453	41.652212
3505.119341	332439.565983	41.657216
3505.152577	332435.920201	41.662221
3504.805825	332415.964796	41.667226
3505.156217	332419.906368	41.672231
3505.079898	332406.527369	41.677236
3504.927767	332397.793768	41.682240
3505.051060	332388.074664	41.687245
3504.883621	332385.529855	41.692250
3505.211068	332371.959725	41.697255
3504.897042	332366.663131	41.702260
3504.684660	332367.969635	41.707264
3504.755389	332360.422796	41.712269
3504.657799	332354.710110	41.717274
3504.845541	332324.181342	41.722279
3504.613786	332330.277079	41.727284
3504.826269	332324.617203	41.732288
3504.747282	332319.690781	41.737293
3504.519635	332306.335687	41.742298
3504.935540	332296.672144	41.747303
3504.977530	332299.287728	41.752308
3505.207477	332283.543576	41.757312
3504.902319	332282.446204	41.762317
3504.803026	332282.461913	41.767322
3504.942365	332258.509028	41.772327
3505.161948	332255.317485	41.777332
3505.087457	332239.799663	41.782336
3504.866308	332234.233792	41.787341
3504.591790	332232.062323	41.792346
3504.816292	332222.047155	41.797351
3504.869208	332212.517363	41.802356
3504.842586	332210.128494	41.807360
3504.599226	332194.128190	41.812365
3504.420149	332184.024070	41.817370
3504.728150	332175.981449	41.822375
3504.688602	332176.802382	41.827380
3504.724360	332181.302876	41.832384
3504.667307	332156.999130	41.837389
3504.771996	332166.020325	41.842394
3504.946445	332160.671949	41.847399
3504.456802	332154.410226	41.852404
3504.751132	332139.368700	41.857408
3504.673982	332142.996002	41.862413
3504.831257	332149.183002	41.867418
3504.730114	332128.068518	41.872423
3504.578504	332118.545589	41.877428
3504.741018	332114.904811	41.882432
3504.948237	332115.330314	41.887437
3504.788828	332108.176250	41.892442
3504.746189	332091.635023	41.897447
3504.917275	332098.940014	41.902452
3504.769054	332075.465323	41.907456
3504.811235	332072.123610	41.912461
3504.639055	332067.313738	41.917466
3504.940485	332059.781312	41.922471
3504.784457	332051.913872	41.927476
3505.152127	332046.051231	41.932480
3504.955513	332034.804231	41.937485
3504.984853	332029.504246	41.942490
3504.837039	332021.788254	41.947495
3504.903272	332007.826558	41.952500
3505.177605	331994.112003	41.957504
3504.999629	331995.565825	41.962509
3504.411210	331969.538471	41.967514
3504.905354	331969.816779	41.972519
3504.597859	331979.819666	41.977524
3504.796470	331962.425598	41.982528
3504.798369	331947.684848	41.987533
3504.628969	331947.482514	41.992538
3504.567050	331948.816155	41.997543
3504.785399	331941.195018	42.002548
3505.044626	331916.357477	42.007552
3504.655131	331921.485305	42.012557
3504.805980	331914.103963	42.017562
3504.739250	331894.384187	42.022567
3504.556125	331897.340877	42.027572
3504.429731	331896.851700	42.032576
3504.421478	331907.571044	42.037581
3504.568310	331891.789030	42.042586
3504.547392	331867.530390	42.047591
3504.325882	331868.812888	42.052596
3504.576541	331875.850736	42.057600
3504.438961	331884.121054	42.062605
3504.512854	331883.116501	42.067610
3504.577603	331862.586717	42.072615
3504.605646	331854.842906	42.077620
3504.517923	331853.074689	42.082624
3504.734727	331859.761473	42.087629
3504.584223	331863.680430	42.092634
3504.670673	331843.019917	42.097639
3504.693135	331836.804497	42.102644
3504.546291	331828.248201	42.107648
3504.525961	331839.631386	42.112653
3504.370243	331820.587580	42.117658
3504.331180	331828.231324	42.122663
3504.825740	331825.989173	42.127668
3504.399676	331821.652217	42.132672
3504.541224	331827.103434	42.137677
3504.639157	331814.867868	42.142682
3504.996810	331797.728661	42.147687
3504.564736	331796.829556	42.152692
3504.787870	331782.588426	42.157696
3504.817467	331773.749643	42.162701
3504.777290	331769.224385	42.167706
3504.965806	331766.495987	42.172711
3504.603440	331753.824011	42.177716
3504.411123	331741.736155	42.182720
3504.633194	331741.701057	42.187725
3504.503781	331754.603556	42.192730
3504.962821	331757.051391	42.197735
3504.602896	331740.051074	42.202740
3504.668232	331723.670902	42.207744
3504.832301	331725.859869	42.212749
3504.588380	331709.452211	42.217754
3504.816659	331691.824260	42.222759
3504.836243	331702.564692	42.227764
3505.077813	331684.323633	42.232768
3504.817920	331671.329939	42.237773
3504.863139	331658.975389	42.242778
3504.831614	331665.905118	42.247783
3504.914344	331649.624014	42.252788
3504.611673	331632.792830	42.257792
3504.516682	331628.810859	42.262797
3504.285720	331643.155113	42.267802
3504.641238	331626.729043	42.272807
3504.250327	331627.707365	42.277812
3504.556318	331623.967503	42.282816
3504.563057	331633.386129	42.287821
3504.488675	331635.969217	42.292826
3504.606492	331609.982833	42.297831
3504.468206	331607.357011	42.302836
3504.471207	331601.653821	42.307840
3504.381561	331601.540711	42.312845
3504.429488	331609.017974	42.317850
3504.779912	331595.902321	42.322855
3504.525624	331587.643027	42.327860
3504.756969	331581.114518	42.332864
3504.822992	331583.217156	42.337869
3504.730098	331576.688990	42.342874
3504.615700	331563.061268	42.347879
3504.447090	331559.141849	42.352884
3504.327976	331549.511874	42.357888
3504.439883	331558.302876	42.362893
3504.407747	331557.340540	42.367898
3504.617426	331543.330618	42.372903
3504.534489	331534.942394	42.377908
3504.252701	331535.597961	42.382912
3504.759164	331538.623855	42.387917
3504.470574	331536.989221	42.392922
3504.622929	331518.507639	42.397927
3504.249259	331507.848640	42.402932
3504.666173	331515.547622	42.407936
3504.627319	331512.167777	42.412941
3504.157785	331522.680059	42.417946
3504.796835	331506.209137	42.422951
3504.531647	331508.796937	42.427956
3504.492738	331491.643976	42.432960
3504.681064	331487.311702	42.437965
3504.495305	331498.670177	42.442970
3504.606321	331479.838699	42.447975
3504.482961	331470.973144	42.452980
3504.527862	331468.547484	42.457984
3504.561954	331468.643940	42.462989
3504.399142	331484.912308	42.467994
3504.596451	331465.710763	42.472999
3504.592360	331458.786667	42.478004
3504.717051	331451.358496	42.483008
3504.598306	331455.654334	42.488013
3504.249478	331450.184964	42.493018
3504.570674	331421.518660	42.498023
3504.246762	331412.939391	42.503028
3504.284826	331427.801246	42.508032
3504.493734	331421.887277	42.513037
3504.224308	331446.013778	42.518042
3504.512258	331432.449717	42.523047
3504.462277	331436.480098	42.528052
3504.719550	331412.711959	42.533056
3504.437852	331407.562935	42.538061
3504.350627	331415.748969	42.543066
3504.838499	331406.634022	42.548071
3504.478733	331410.178748	42.553076
3504.717672	331382.696531	42.558080
3504.365942	331378.475090	42.563085
3504.718869	331376.051648	42.568090
3504.814625	331373.414276	42.573095
3504.523040	331362.462233	42.578100
3504.413470	331355.376592	42.583104
3504.530020	331353.983407	42.588109
3504.512306	331364.551574	42.593114
3504.751297	331363.444537	42.598119
3504.584686	331342.009212	42.603124
3504.591769	331340.200536	42.608128
3505.040120	331332.390221	42.613133
3504.690137	331325.520796	42.618138
3504.633068	331298.721812	42.623143
3504.441980	331294.220383	42.628148
3504.671764	331299.504936	42.633152
3505.002985	331300.369097	42.638157
3504.549882	331279.055421	42.643162
3504.594297	331262.882124	42.648167
3504.588767	331264.435991	42.653172
3504.761989	331272.911829	42.658176
3504.766651	331260.283577	42.663181
3504.403447	331260.850183	42.668186
3504.557061	331259.985770	42.673191
3504.594671	331261.049102	42.678196
3504.863349	331237.635525	42.683200
3504.526488	331235.448423	42.688205
3504.310591	331228.226827	42.693210
3504.580387	331230.831893	42.698215
3504.501745	331238.609250	42.703220
3504.636028	331226.724262	42.708224
3504.833701	331212.639799	42.713229
3504.434481	331205.421724	42.718234
3504.742907	331208.071601	42.723239
3504.643896	331193.804910	42.728244
3504.998800	331170.123092	42.733248
3505.041698	331168.843383	42.738253
3504.509549	331170.302297	42.743258
3504.728461	331146.081878	42.748263
3504.509650	331136.976785	42.753268
3504.469983	331140.496377	42.758272
3504.536849	331148.250740	42.763277
3504.413745	331126.401133	42.768282
3504.756694	331126.499678	42.773287
3504.370097	331121.570889	42.778292
3504.645469	331111.318397	42.783296
3504.423013	331117.183636	42.788301
3504.124117	331107.862071	42.793306
3504.653171	331094.921759	42.798311
3504.415228	331099.058250	42.803316
3504.396461	331091.067171	42.808321
3504.447591	331101.879080	42.813325
3504.436805	331096.279865	42.818330
3504.616971	331081.638051	42.823335
3504.279355	331078.076290	42.828340
3504.574162	331066.089522	42.833345
3504.886516	331060.897475	42.838349
3504.120021	331077.948760	42.843354
3504.225484	331078.237603	42.848359
3504.352093	331069.790739	42.853364
3504.285080	331062.469212	42.858369
3504.319833	331053.374940	42.863373
3504.255234	331048.064275	42.868378
3504.474077	331043.472563	42.873383
3504.307491	331057.272119	42.878388
3504.295915	331057.910430	42.883393
3504.668693	331051.232220	42.888397
3504.270840	331038.794859	42.893402
3504.600386	331019.521374	42.898407
3504.552378	331026.861111	42.903412
3504.294221	331030.135203	42.908417
3504.440062	331025.300443	42.913421
3504.374807	331035.468833	42.918426
3504.509586	331024.092910	42.923431
3504.072950	331019.401154	42.928436
3504.139196	331006.050276	42.933441
3504.445533	331009.973431	42.938445
3503.939249	331015.705338	42.943450
3504.232471	331009.268831	42.948455
3504.329462	331015.465457	42.953460
3504.498051	331013.325734	42.958465
3504.672401	331012.534417	42.963469
3504.271560	331009.033565	42.968474
3504.168863	330991.534148	42.973479
3504.366999	330987.454883	42.978484
3504.389589	330986.713017	42.983489
3504.710118	330984.880237	42.988493
3504.275572	331000.326072	42.993498
3504.382090	330997.126891	42.998503
3504.315234	330998.384953	43.003508
3504.329607	330978.601191	43.008513
3504.220720	330978.669334	43.013517
3504.333991	330987.281977	43.018522
3504.652913	330979.695757	43.023527
3504.325864	330972.720838	43.028532
3504.514838	330980.634125	43.033537
3504.772789	330976.621780	43.038541
3504.564285	330960.717530	43.043546
3504.765870	330950.782187	43.048551
3504.456370	330960.047224	43.053556
3504.671041	330945.399928	43.058561
3504.668764	330926.280714	43.063565
3504.557253	330923.396046	43.068570
3504.544178	330919.375627	43.073575
3504.631174	330930.640150	43.078580
3504.229171	330910.005678	43.083585
3504.416251	330900.632716	43.088589
3504.335785	330902.987662	43.093594
3504.622650	330892.325981	43.098599
3504.536910	330904.559794	43.103604
3504.420242	330901.930530	43.108609
3504.785914	330886.495585	43.113613
3504.264875	330883.090106	43.118618
3504.763830	330879.854337	43.123623
3504.523365	330892.850920	43.128628
3504.264842	330881.562613	43.133633
3504.758304	330864.605387	43.138637
3504.487525	330860.549330	43.143642
3504.837496	330843.080149	43.148647
3504.420137	330847.601444	43.153652
3504.632015	330849.782880	43.158657
3504.520056	330827.422245	43.163661
3504.207926	330824.925714	43.168666
3504.574436	330827.744635	43.173671
3504.361057	330826.785483	43.178676
3504.541711	330820.850475	43.183681
3504.504636	330822.332962	43.188685
3504.586612	330811.601826	43.193690
3504.410643	330804.348417	43.198695
3504.826594	330782.642616	43.203700
3504.495754	330787.710332	43.208705
3504.271050	330786.905724	43.213709
3504.026279	330780.605169	43.218714
3504.263542	330764.477650	43.223719
3504.054385	330776.018147	43.228724
3504.349410	330775.666009	43.233729
3504.462456	330766.355653	43.238733
3504.422749	330778.123949	43.243738
3504.419764	330782.121477	43.248743
3504.523718	330786.585818	43.253748
3504.489694	330767.700711	43.258753
3504.596778	330754.827050	43.263757
3504.212225	330757.510123	43.268762
3504.364236	330750.255775	43.273767
3504.135229	330758.489756	43.278772
3504.605662	330753.119943	43.283777
3504.608759	330750.420821	43.288781
3504.300341	330735.372462	43.293786
3504.685277	330723.498684	43.298791
3504.510858	330730.272880	43.303796
3504.609570	330725.674682	43.308801
3504.360969	330732.104181	43.313805
3504.093430	330723.770508	43.318810
3504.126118	330698.280979	43.323815
3504.139196	330697.464237	43.328820
3503.858761	330704.891669	43.333825
3504.289944	330690.337388	43.338829
3504.065386	330709.467088	43.343834
3504.063745	330711.427694	43.348839
3503.864850	330713.088520	43.353844
3503.905762	330710.408877	43.358849
3504.008235	330710.189016	43.363853
3503.949126	330714.195421	43.368858
3504.399754	330720.565294	43.373863
3504.517723	330720.801244	43.378868
3504.597156	330717.071696	43.383873
3504.418363	330731.102373	43.388877
3504.394556	330725.708859	43.393882
3504.531068	330713.594306	43.398887
3504.240985	330711.705300	43.403892
3504.406291	330705.721791	43.408897
3504.496668	330696.745975	43.413901
3503.912223	330717.612858	43.418906
3504.370991	330691.495870	43.423911
3504.192572	330721.336477	43.428916
3504.378251	330705.268018	43.433921
3504.096884	330724.814038	43.438925
3504.295947	330718.697898	43.443930
3504.484847	330705.938589	43.448935
3503.946777	330688.660684	43.453940
3504.207541	330684.164158	43.458945
3504.539343	330687.294078	43.463949
3504.545359	330683.321546	43.468954
3504.692723	330684.367534	43.473959
3504.290106	330682.929120	43.478964
3504.376036	330675.023279	43.483969
3504.413963	330671.198455	43.488973
3504.017171	330669.122647	43.493978
3504.504805	330657.843637	43.498983
3504.223639	330665.118435	43.503988
3504.353709	330670.953436	43.508993
3504.622016	330662.585959	43.513997
3504.669953	330661.229068	43.519002
3504.719062	330644.240207	43.524007
3504.650203	330632.158108	43.529012
3504.483650	330633.941117	43.534017
3504.723182	330631.382824	43.539021
3504.231089	330631.358796	43.544026
3504.356627	330611.939245	43.549031
3504.505815	330606.441997	43.554036
3504.651781	330605.196901	43.559041
3504.583566	330600.956052	43.564045
3504.386813	330612.596449	43.569050
3504.324184	330574.697980	43.574055
3504.316149	330573.120806	43.579060
3504.063382	330583.344361	43.584065
3504.107877	330577.125352	43.589069
3504.131548	330583.562737	43.594074
3504.526063	330583.627672	43.599079
3504.316679	330594.251710	43.604084
3504.483203	330585.162007	43.609089
3505.025424	330579.984504	43.614093
3504.491893	330560.236332	43.619098
3504.427646	330556.911376	43.624103
3504.342134	330565.020856	43.629108
3504.449198	330564.774810	43.634113
3504.832228	330552.010242	43.639117
3504.294989	330537.252609	43.644122
3504.479120	330528.567458	43.649127
3504.527267	330528.152513	43.654132
3504.498167	330530.779399	43.659137
3504.736104	330525.599081	43.664141
3503.945716	330513.350984	43.669146
3504.268636	330502.225285	43.674151
3504.271592	330507.927641	43.679156
3503.908443	330515.342710	43.684161
3504.392870	330513.331253	43.689165
3503.776246	330519.971706	43.694170
3504.516947	330510.714842	43.699175
3504.556427	330522.801627	43.704180
3504.505811	330517.717844	43.709185
3504.696336	330503.125197	43.714189
3504.371572	330497.728328	43.719194
3504.476280	330482.156343	43.724199
3504.130621	330487.633766	43.729204
3503.937688	330490.337472	43.734209
3504.027887	330487.930078	43.739213
3504.035538	330495.337445	43.744218
3504.485450	330497.124833	43.749223
3504.413187	330505.945077	43.754228
3504.119698	330506.067864	43.759233
3504.559201	330473.869148	43.764237
3504.258174	330474.705978	43.769242
3504.326150	330461.252893	43.774247
3504.499429	330470.899928	43.779252
3504.433048	330470.808597	43.784257
3504.378816	330481.280828	43.789261
3504.183841	330473.852178	43.794266
3504.309791	330464.514285	43.799271
3504.238966	330452.890730	43.804276
3504.346531	330444.955985	43.809281
3504.648346	330446.283067	43.814285
3503.910143	330455.743238	43.819290
3504.522248	330444.189927	43.824295
3504.445512	330455.378571	43.829300
3504.285652	330463.397981	43.834305
3504.618337	330446.924341	43.839309
3504.290646	330439.032948	43.844314
3504.243680	330420.862652	43.849319
3503.923798	330423.815562	43.854324
3504.065987	330427.662863	43.859329
3504.355049	330423.747405	43.864333
3504.359786	330429.271272	43.869338
3504.567064	330437.792740	43.874343
3504.523447	330435.330123	43.879348
3504.188962	330414.430248	43.884353
3504.505486	330404.807628	43.889357
3504.074323	330402.533574	43.894362
3504.397197	330390.847768	43.899367
3504.537780	330403.427768	43.904372
3504.580317	330398.914808	43.909377
3504.520038	330396.505741	43.914381
3504.294579	330394.326461	43.919386
3504.290899	330376.072933	43.924391
3504.258260	330373.353988	43.929396
3504.242159	330378.957531	43.934401
3504.672207	330372.422960	43.939405
3504.201104	330384.055848	43.944410
3504.327632	330380.140625	43.949415
3504.276562	330378.264741	43.954420
3504.305967	330365.937934	43.959425
3504.531371	330350.143167	43.964429
3504.273976	330349.114591	43.969434
3504.385068	330340.873770	43.974439
3504.466991	330352.266478	43.979444
3504.602013	330353.747226	43.984449
3504.437229	330352.220287	43.989453
3503.868061	330332.935951	43.994458
3504.370894	330328.859397	43.999463
3504.443190	330332.794130	44.004468
3504.243954	330335.600675	44.009473
3504.414864	330319.865435	44.014477
3504.397702	330337.154850	44.019482
3504.455222	330335.134503	44.024487
3504.187061	330344.749508	44.029492
3504.434380	330319.684180	44.034497
3504.275036	330298.578370	44.039501
3504.186999	330299.177858	44.044506
3504.523865	330300.932205	44.049511
3504.558251	330299.322859	44.054516
3504.467619	330297.555064	44.059521
3504.787763	330303.232749	44.064525
3504.344633	330292.635473	44.069530
3504.693547	330269.208905	44.074535
3504.597329	330269.606013	44.079540
3504.487048	330269.267032	44.084545
3504.739939	330246.466655	44.089549
3504.495807	330239.198508	44.094554
3504.798303	330238.234170	44.099559
3504.514274	330226.542450	44.104564
3504.444960	330232.154416	44.109569
3504.352026	330216.868212	44.114573
3503.970752	330214.586265	44.119578
3504.224964	330197.972222	44.124583
3504.047412	330203.193956	44.129588
3504.120415	330203.538853	44.134593
3504.426578	330210.873596	44.139597
3504.300631	330217.894766	44.144602
3504.304091	330208.347073	44.149607
3504.173014	330214.325233	44.154612
3504.331651	330205.847748	44.159617
3504.523542	330215.008151	44.164621
3504.351533	330192.936869	44.169626
3504.559353	330171.034663	44.174631
3504.254383	330184.143404	44.179636
3504.287257	330184.825613	44.184641
3504.453698	330173.342718	44.189645
3504.059704	330182.773964	44.194650
3504.385820	330197.666904	44.199655
3504.763326	330190.122261	44.204660
3504.173789	330163.279751	44.209665
3504.184191	330150.141220	44.214669
3504.000019	330150.908662	44.219674
3504.441807	330158.705691	44.224679
3504.258572	330170.649529	44.229684
3504.095027	330158.429569	44.234689
3504.220341	330154.463607	44.239693
3503.843842	330180.847849	44.244698
3504.160259	330160.048671	44.249703
3504.484175	330173.236204	44.254708
3504.410475	330168.487015	44.259713
3504.386578	330142.446142	44.264717
3504.475631	330137.365711	44.269722
3504.358773	330140.693881	44.274727
3504.395239	330134.043299	44.279732
3504.160060	330142.812965	44.284737
3504.713525	330136.971717	44.289741
3504.347873	330143.139722	44.294746
3504.449220	330118.173781	44.299751
3504.445092	330121.382293	44.304756
3504.450994	330121.992390	44.309761
3504.358624	330119.079206	44.314765
3504.264471	330123.905874	44.319770
3504.560159	330123.808220	44.324775
3504.382141	330102.654389	44.329780
3504.169516	330096.145021	44.334785
3504.162836	330083.696575	44.339789
3504.073928	330090.024505	44.344794
3504.431329	330087.116591	44.349799
3504.508260	330096.626152	44.354804
3504.587633	330094.245916	44.359809
3504.659071	330090.033877	44.364813
3504.149589	330079.828947	44.369818
3504.484837	330055.691618	44.374823
3504.198051	330055.736968	44.379828
3504.226672	330065.381466	44.384833
3504.187048	330067.577227	44.389837
3504.156616	330070.331635	44.394842
3504.073446	330071.745047	44.399847
3504.346457	330073.254903	44.404852
3504.267902	330070.823256	44.409857
3504.854518	330061.361565	44.414861
3504.493179	330049.656581	44.419866
3504.331755	330036.112390	44.424871
3504.437374	330033.015146	44.429876
3504.483937	330050.116339	44.434881
3504.523262	330031.575878	44.439885
3504.239412	330027.801892	44.444890
3504.321655	330007.217908	44.449895
3504.281316	330011.756025	44.454900
3504.294073	330004.498160	44.459905
3504.573567	330011.302497	44.464909
3504.028017	330017.957217	44.469914
3504.277187	330008.981674	44.474919
3504.089969	330014.994183	44.479924
3504.204420	330023.708588	44.484929
3504.239556	330026.630846	44.489933
3503.951971	330029.145860	44.494938
3504.210419	330030.047000	44.499943
3504.027933	330008.104615	44.504948
3504.175745	329997.133821	44.509953
3504.462001	329982.984202	44.514957
3503.953934	329992.051619	44.519962
3504.315775	329986.826215	44.524967
3504.583592	329986.758427	44.529972
3504.565422	329988.568910	44.534977
3504.223814	329987.910071	44.539981
3504.388628	329995.267182	44.544986
3504.304783	329976.287914	44.549991
3504.119832	329971.938189	44.554996
3504.052552	329969.428379	44.560001
3504.248222	329963.414551	44.565005
3504.001559	329971.320441	44.570010
3504.219993	329965.455769	44.575015
3504.445357	329972.395963	44.580020
3504.255003	329974.971984	44.585025
3504.206353	329966.909131	44.590029
3504.208868	329973.910014	44.595034
3504.416850	329969.396331	44.600039
3504.412827	329974.336056	44.605044
3504.359416	329952.704218	44.610049
3504.632347	329941.739095	44.615053
3503.934165	329947.246830	44.620058
3504.222011	329936.355725	44.625063
3504.281317	329930.999932	44.630068
3504.275958	329939.224105	44.635073
3504.238135	329940.579431	44.640077
3503.918598	329944.270621	44.645082
3504.455180	329941.334374	44.650087
3504.096354	329956.055597	44.655092
3504.086597	329967.793827	44.660097
3504.378213	329948.042337	44.665101
3504.063250	329946.691888	44.670106
3503.934755	329925.453800	44.675111
3504.217583	329913.977924	44.680116
3504.209945	329929.432866	44.685121
3504.364853	329924.087418	44.690125
3504.160680	329921.777463	44.695130
3504.305204	329924.606053	44.700135
3504.147529	329926.795022	44.705140
3504.154156	329930.714699	44.710145
3504.319234	329940.821365	44.715149
3504.326537	329931.120274	44.720154
3504.410287	329937.853727	44.725159
3504.384667	329930.169116	44.730164
3504.446552	329907.678885	44.735169
3504.230718	329906.032712	44.740173
3504.148713	329900.011859	44.745178
3504.459849	329899.809926	44.750183
3504.552184	329903.614217	44.755188
3504.317872	329904.771476	44.760193
3504.516697	329897.127756	44.765197
3504.318198	329891.889096	44.770202
3504.331496	329885.700421	44.775207
3504.381654	329873.421169	44.780212
3504.147482	329868.697331	44.785217
3504.670467	329867.468997	44.790221
3504.331118	329879.132051	44.795226
3504.676156	329865.355005	44.800231
3504.204075	329852.649130	44.805236
3504.128227	329858.083942	44.810241
3504.105101	329847.878468	44.815245
3504.325357	329845.552329	44.820250
3504.385920	329848.368737	44.825255
3504.482233	329849.295512	44.830260
3504.276066	329846.858574	44.835265
3504.559352	329848.545024	44.840269
3504.256505	329828.836567	44.845274
3504.568025	329811.678734	44.850279
3504.571977	329815.242411	44.855284
3504.571620	329821.556364	44.860289
3504.539634	329810.919479	44.865293
3504.408395	329808.954419	44.870298
3504.420206	329777.306745	44.875303
3504.301821	329775.390570	44.880308
3504.086353	329785.786552	44.885313
3504.202662	329787.906750	44.890317
3503.972973	329791.507365	44.895322
3504.041666	329794.602542	44.900327
3504.284048	329793.393109	44.905332
3504.232571	329804.730612	44.910337
3503.998753	329782.465307	44.915341
3503.881786	329801.705526	44.920346
3504.030992	329791.141829	44.925351
3504.000342	329791.706788	44.930356
3503.962585	329788.555824	44.935361
3504.583538	329800.754471	44.940365
3504.175054	329806.318253	44.945370
3504.384853	329794.013750	44.950375
3504.504136	329791.627195	44.955380
3504.457718	329780.814373	44.960385
3504.336485	329767.467453	44.965389
3504.239204	329772.625609	44.970394
3504.568636	329774.304766	44.975399
3504.252126	329777.817271	44.980404
3504.321792	329772.510747	44.985409
3504.315840	329753.289976	44.990413
3503.984590	329745.755502	44.995418
3504.178366	329739.461904	45.000423
3503.999247	329738.242730	45.005428
3503.880178	329748.699855	45.010433
3504.445439	329736.950167	45.015437
3503.925965	329738.738074	45.020442
3504.257393	329735.503282	45.025447
3504.265130	329749.708327	45.030452
3504.158603	329749.979772	45.035457
3504.210585	329745.643494	45.040461
3504.026368	329755.296221	45.045466
3504.119883	329759.202170	45.050471
3504.309944	329763.576581	45.055476
3504.288815	329760.422987	45.060481
3504.350773	329761.126061	45.065485
3504.106534	329764.728978	45.070490
3504.006385	329754.077402	45.075495
3504.078559	329741.820107	45.080500
3504.040583	329739.000146	45.085505
3504.244599	329726.009147	45.090509
3504.144023	329741.198769	45.095514
3504.356460	329736.862582	45.100519
3504.389426	329736.144522	45.105524
3504.058788	329745.947696	45.110529
3504.242354	329746.937055	45.115533
3503.970143	329748.202145	45.120538
3504.299905	329743.083633	45.125543
3504.194804	329751.272676	45.130548
3504.018037	329746.488836	45.135553
3504.339752	329743.484714	45.140557
3504.338869	329765.710780	45.145562
3504.248736	329754.370220	45.150567
3504.466696	329735.368638	45.155572
3504.172360	329721.030707	45.160577
3504.447539	329716.735518	45.165581
3504.329630	329725.435774	45.170586
3504.977015	329707.664716	45.175591
3504.697549	329719.292869	45.180596
3504.357408	329698.775577	45.185601
3504.777102	329681.473317	45.190605
3504.306446	329691.171337	45.195610
3504.404120	329687.515232	45.200615
3504.502894	329688.492538	45.205620
3504.360491	329663.132175	45.210625
3504.425613	329658.411925	45.215629
3504.138862	329653.365416	45.220634
3504.015590	329651.297255	45.225639
3503.919870	329659.128395	45.230644
3503.716150	329649.206037	45.235649
3504.286646	329654.716896	45.240653
3504.233069	329664.196226	45.245658
3504.321584	329662.451012	45.250663
3504.509471	329649.335254	45.255668
3504.121146	329664.035738	45.260673
3504.265399	329660.346808	45.265677
3504.122071	329667.879963	45.270682
3504.283781	329650.338430	45.275687
3504.142135	329638.318597	45.280692
3504.027013	329638.387726	45.285697
3504.125867	329634.833269	45.290701
3504.063141	329642.430061	45.295706
3503.982594	329634.830482	45.300711
3504.106956	329641.124733	45.305716
3504.314754	329646.336503	45.310721
3504.462161	329641.017680	45.315725
3504.427092	329648.279129	45.320730
3503.968027	329643.565372	45.325735
3504.134863	329642.189665	45.330740
3504.147398	329645.344644	45.335745
3504.652222	329651.476908	45.340749
3504.368307	329640.243346	45.345754
3504.359712	329616.211154	45.350759
3504.363789	329620.844110	45.355764
3504.051619	329619.671427	45.360769
3504.164630	329612.932321	45.365773
3504.144266	329621.846301	45.370778
3503.979687	329614.972864	45.375783
3504.208560	329609.666619	45.380788
3504.163869	329620.799403	45.385793
3504.127004	329611.258010	45.390797
3504.124138	329622.002293	45.395802
3504.175530	329623.598114	45.400807
3504.281199	329622.944937	45.405812
3504.105732	329625.009431	45.410817
3504.186881	329625.607635	45.415821
3503.989468	329629.432289	45.420826
3504.400239	329620.609366	45.425831
3504.538711	329611.193008	45.430836
3504.199827	329603.888861	45.435841
3504.460673	329587.299093	45.440845
3504.410270	329590.082136	45.445850
3504.236151	329603.959529	45.450855
3504.330281	329600.634950	45.455860
3504.431058	329600.466273	45.460865
3504.422511	329566.912283	45.465869
3504.064431	329577.356299	45.470874
3504.235989	329566.305310	45.475879
3504.230287	329556.784443	45.480884
3504.030046	329568.043663	45.485889
3504.384219	329558.058553	45.490893
3504.515072	329568.374354	45.495898
3504.351549	329564.937752	45.500903
3504.396449	329567.552972	45.505908
3504.390980	329565.237051	45.510913
3504.427870	329545.347512	45.515917
3504.105881	329545.194753	45.520922
3504.345203	329536.653519	45.525927
3504.236390	329545.428735	45.530932
3503.843861	329550.124397	45.535937
3504.367689	329541.945533	45.540941
3504.097963	329549.524142	45.545946
3504.380022	329553.069323	45.550951
3504.302905	329549.720897	45.555956
3504.172205	329556.386450	45.560961
3504.499609	329531.537332	45.565965
3504.117013	329528.109903	45.570970
3504.327563	329512.775577	45.575975
3504.556983	329507.902047	45.580980
3504.193105	329524.609980	45.585985
3504.471525	329510.996157	45.590989
3504.316219	329512.115472	45.595994
3504.541835	329501.666951	45.600999
3504.344511	329487.720988	45.606004
3504.241388	329496.062502	45.611009
3504.498600	329485.608984	45.616013
3504.114766	329495.395140	45.621018
3504.102030	329483.303984	45.626023
3504.484362	329482.301555	45.631028
3504.377912	329490.643595	45.636033
3504.605576	329487.170604	45.641037
3504.438854	329455.831074	45.646042
3504.230086	329456.704248	45.651047
3504.367750	329456.071471	45.656052
3504.487265	329451.444446	45.661057
3504.645346	329448.848072	45.666061
3504.165103	329447.880174	45.671066
3504.091588	329445.371332	45.676071
3504.042947	329436.035453	45.681076
3504.009036	329449.101469	45.686081
3504.262197	329444.784286	45.691085
3504.109266	329427.190608	45.696090
3503.933454	329431.037316	45.701095
3503.948214	329425.153883	45.706100
3503.712128	329423.332686	45.711105
3504.235776	329438.729194	45.716109
3503.808026	329448.293165	45.721114
3503.942896	329464.489453	45.726119
3504.357193	329460.401390	45.731124
3504.392189	329454.718436	45.736129
3504.238162	329434.375323	45.741133
3504.109924	329438.570940	45.746138
3504.343154	329426.033539	45.751143
3504.411391	329434.857156	45.756148
3504.378212	329443.034862	45.761153
3504.774910	329439.789738	45.766157
3504.250010	329427.754084	45.771162
3503.972245	329402.796924	45.776167
3504.258909	329408.810941	45.781172
3504.178297	329408.238131	45.786177
3504.045253	329405.229513	45.791181
3503.971631	329411.071355	45.796186
3504.148805	329410.406872	45.801191
3504.265967	329409.344526	45.806196
3503.934661	329424.570689	45.811201
3504.363285	329409.481919	45.816205
3504.244646	329415.509093	45.821210
3504.153755	329410.355225	45.826215
3504.352806	329415.593853	45.831220
3504.319833	329420.309057	45.836225
3504.421086	329411.229530	45.841229
3504.227274	329394.482466	45.846234
3504.327292	329376.568732	45.851239
3504.315189	329383.673819	45.856244
3503.876056	329389.700746	45.861249
3504.247558	329381.800540	45.866253
3504.259601	329388.850890	45.871258
3504.126420	329381.641497	45.876263
3504.492019	329388.355899	45.881268
3504.115132	329391.394239	45.886273
3504.437512	329398.090014	45.891277
3504.055472	329403.267754	45.896282
3504.519111	329386.773179	45.901287
3504.256152	329372.761193	45.906292
3504.221087	329352.933898	45.911297
3504.431207	329347.070493	45.916301
3504.471305	329353.810899	45.921306
3504.068248	329358.711912	45.926311
3504.460773	329350.451948	45.931316
3504.097574	329360.463994	45.936321
3504.332438	329361.827140	45.941325
3504.147187	329350.374261	45.946330
3504.028535	329343.824511	45.951335
3504.037131	329334.683246	45.956340
3503.902524	329348.528979	45.961345
3504.299731	329326.876640	45.966349
3503.932314	329331.313752	45.971354
3504.316122	329345.077527	45.976359
3504.169679	329339.066817	45.981364
3504.217540	329339.084721	45.986369
3504.266903	329343.124969	45.991373
3504.200298	329334.555699	45.996378
3504.431115	329331.973281	46.001383
3504.256014	329331.593624	46.006388
3503.986514	329342.609234	46.011393
3504.149104	329341.997975	46.016397
3504.113133	329347.477438	46.021402
3504.327701	329349.989465	46.026407
3504.323904	329343.879826	46.031412
3504.247581	329336.177711	46.036417
3504.377798	329310.926886	46.041421
3504.230836	329312.630450	46.046426
3503.918347	329311.941542	46.051431
3504.339238	329304.160817	46.056436
3503.943611	329319.218954	46.061441
3504.137646	329301.824986	46.066445
3504.246591	329310.693100	46.071450
3504.325025	329304.697755	46.076455
3504.414269	329320.112045	46.081460
3504.542212	329318.462429	46.086465
3504.347972	329298.583906	46.091469
3504.172415	329291.966770	46.096474
3504.574530	329277.365893	46.101479
3504.427242	329285.230683	46.106484
3504.291493	329286.321450	46.111489
3504.502512	329289.801497	46.116493
3504.375979	329292.672964	46.121498
3504.201816	329277.017521	46.126503
3503.944722	329256.639736	46.131508
3503.898873	329250.002090	46.136513
3504.310470	329244.335959	46.141517
3504.191076	329263.474861	46.146522
3504.306698	329256.557093	46.151527
3504.206199	329253.365107	46.156532
3503.898400	329257.538204	46.161537
3504.213945	329254.433199	46.166541
3504.121497	329262.976727	46.171546
3503.757122	329262.805209	46.176551
3504.055944	329263.623597	46.181556
3504.050991	329261.154829	46.186561
3504.390504	329252.597723	46.191565
3504.227991	329259.599304	46.196570
3503.906694	329267.848038	46.201575
3504.448690	329253.556014	46.206580
3503.725005	329270.626399	46.211585
3504.068340	329260.057397	46.216589
3504.017873	329262.305814	46.221594
3503.950400	329263.869516	46.226599
3504.127104	329275.883887	46.231604
3503.925499	329272.835184	46.236609
3504.225209	329267.899607	46.241613
3504.337385	329273.763005	46.246618
3504.438355	329269.520792	46.251623
3504.426817	329254.985307	46.256628
3504.343018	329241.606917	46.261633
3504.692508	329235.568714	46.266637
3504.490512	329243.187564	46.271642
3504.371608	329237.019736	46.276647
3504.428634	329243.935691	46.281652
3504.153193	329236.239587	46.286657
3504.542267	329212.424451	46.291661
3504.082730	329215.985053	46.296666
3503.942832	329218.323988	46.301671
3504.240955	329200.047921	46.306676
3504.173109	329209.733239	46.311681
3504.600014	329202.919011	46.316685
3504.553918	329207.992735	46.321690
3504.516378	329218.997150	46.326695
3504.628530	329192.145198	46.331700
3504.130073	329187.284884	46.336705
3504.469755	329173.432180	46.341709
3504.103894	329183.699264	46.346714
3504.055751	329184.317913	46.351719
3504.377551	329188.111422	46.356724
3504.369104	329188.418282	46.361729
3504.344530	329178.518459	46.366733
3504.493900	329192.268407	46.371738
3504.228790	329169.549599	46.376743
3504.023584	329158.099846	46.381748
3503.999173	329151.102370	46.386753
3504.608733	329146.550610	46.391757
3504.003329	329166.428317	46.396762
3504.108454	329155.260474	46.401767
3504.363768	329145.163641	46.406772
3504.244191	329154.500712	46.411777
3504.500158	329150.972313	46.416781
3504.371399	329155.957271	46.421786
3504.322409	329149.040059	46.426791
3504.346105	329130.247253	46.431796
3503.927675	329133.877738	46.436801
3504.528691	329124.006303	46.441805
3504.451463	329124.604090	46.446810
3504.177804	329126.174932	46.451815
3504.310582	329115.308225	46.456820
3504.292004	329123.407279	46.461825
3504.253278	329113.535145	46.466829
3504.077654	329135.992696	46.471834
3503.937374	329123.794350	46.476839
3504.196188	329131.696792	46.481844
3503.942870	329123.233395	46.486849
3504.222816	329112.343421	46.491853
3504.158144	329098.325495	46.496858
3503.708802	329109.114976	46.501863
3504.047922	329106.820942	46.506868
3504.068255	329110.127467	46.511873
3504.253361	329097.444864	46.516877
3504.119531	329112.003382	46.521882
3503.896833	329107.532277	46.526887
3504.421947	329093.624784	46.531892
3503.827543	329110.063739	46.536897
3503.613462	329093.167056	46.541901
3503.909757	329117.968653	46.546906
3503.905687	329124.868819	46.551911
3504.207486	329128.105386	46.556916
3504.101927	329125.652519	46.561921
3504.451807	329106.426247	46.566925
3504.342125	329113.368570	46.571930
3504.610736	329108.947088	46.576935
3504.644135	329105.683009	46.581940
3504.453981	329115.514972	46.586945
3504.727934	329096.071566	46.591949
3504.742216	329087.133048	46.596954
3504.176177	329101.530764	46.601959
3504.172206	329086.866753	46.606964
3504.189204	329082.001319	46.611969
3504.339002	329084.396297	46.616973
3504.082811	329089.732379	46.621978
3503.968941	329086.644337	46.626983
3504.422040	329081.709958	46.631988
3504.137209	329075.644727	46.636993
3504.573818	329055.386353	46.641997
3503.949545	329052.837273	46.647002
3503.949009	329051.233422	46.652007
3504.387036	329044.570178	46.657012
3504.564482	329047.902787	46.662017
3504.685334	329054.477696	46.667021
3504.206991	329062.598523	46.672026
3504.279161	329048.457117	46.677031
3504.567665	329029.011394	46.682036
3504.227207	329032.909611	46.687041
3504.099125	329021.753158	46.692045
3503.994541	329015.302994	46.697050
3503.869611	329039.050993	46.702055
3504.073346	329020.815265	46.707060
3504.130589	329032.441210	46.712065
3504.251305	329027.253861	46.717069
3503.813570	329021.085502	46.722074
3504.033763	329030.190656	46.727079
3504.191466	329024.386433	46.732084
3504.204084	329032.455105	46.737089
3504.366765	329023.518577	46.742093
3504.433929	329026.410351	46.747098
3504.584409	329035.959337	46.752103
3504.381772	329013.688876	46.757108
3503.978043	329007.642437	46.762113
3504.551734	328998.233577	46.767117
3503.994763	329007.079707	46.772122
3504.109926	329009.047351	46.777127
3504.235559	329004.597549	46.782132
3504.215020	329009.998219	46.787137
3504.549514	329003.376799	46.792141
3504.275691	329004.565777	46.797146
3504.233047	329010.708267	46.802151
3504.334606	329005.574864	46.807156
3503.910992	328991.868261	46.812161
3504.266731	328981.399098	46.817165
3503.929725	328974.400106	46.822170
3504.087346	328975.648173	46.827175
3503.890967	328979.167182	46.832180
3503.802885	328976.686087	46.837185
3504.222796	328985.505077	46.842189
3504.149618	328979.966486	46.847194
3503.757042	328977.177098	46.852199
3504.075878	328976.642972	46.857204
3503.944708	328986.542005	46.862209
3504.296252	328988.726874	46.867213
3504.181147	328986.250052	46.872218
3503.909830	328983.645169	46.877223
3504.197535	328988.080566	46.882228
3504.089024	328984.431565	46.887233
3504.257005	328985.728913	46.892237
3504.210231	328985.532642	46.897242
3503.897814	328984.105394	46.902247
3504.401038	328983.211144	46.907252
3503.979746	328996.847670	46.912257
3504.231263	328984.943792	46.917261
3504.028917	329000.022354	46.922266
3504.158666	328994.375305	46.927271
3504.556774	328988.991342	46.932276
3504.238611	329005.717621	46.937281
3504.408345	328989.243965	46.942285
3504.384669	328981.762627	46.947290
3504.369956	328966.998454	46.952295
3504.289693	328966.527423	46.957300
3504.434332	328959.732339	46.962305
3504.596398	328958.026401	46.967309
3504.284620	328967.597557	46.972314
3504.456408	328961.867480	46.977319
3504.466054	328937.908569	46.982324
3504.286780	328935.034537	46.987329
3504.320227	328927.289568	46.992333
3504.333550	328936.809331	46.997338
3504.244204	328946.319864	47.002343
3504.409463	328937.255622	47.007348
3504.296364	328943.078282	47.012353
3504.221285	328933.491927	47.017357
3504.079953	328914.699698	47.022362
3503.973154	328913.494537	47.027367
3504.311928	328901.016742	47.032372
3503.755309	328907.444173	47.037377
3503.901752	328906.733625	47.042381
3503.846414	328911.325098	47.047386
3504.352684	328914.631186	47.052391
3504.389732	328912.766795	47.057396
3504.205407	328909.358911	47.062401
3504.374527	328909.561321	47.067405
3503.767048	328919.357449	47.072410
3504.015902	328924.715535	47.077415
3504.277423	328908.991136	47.082420
3504.142074	328917.032294	47.087425
3504.344585	328910.100759	47.092429
3504.293695	328911.101737	47.097434
3503.956169	328914.337549	47.102439
3504.120272	328920.880172	47.107444
3503.979497	328920.138653	47.112449
3504.021647	328921.252219	47.117453
3504.093571	328928.267685	47.122458
3504.216042	328909.713805	47.127463
3504.407501	328913.858908	47.132468
3504.200003	328914.069940	47.137473
3504.157409	328891.163113	47.142477
3504.252203	328885.572501	47.147482
3503.822866	328898.802964	47.152487
3503.925372	328884.045702	47.157492
3503.938040	328892.038002	47.162497
3504.140420	328884.673673	47.167501
3504.056149	328889.015127	47.172506
3504.028165	328893.729575	47.177511
3504.306271	328884.367431	47.182516
3504.117643	328889.998359	47.187521
3503.918169	328881.831938	47.192525
3504.240146	328896.063841	47.197530
3504.083467	328898.634575	47.202535
3504.209090	328900.498730	47.207540
3503.810959	328907.384836	47.212545
3504.055487	328901.032226	47.217549
3504.224820	328889.574139	47.222554
3504.238026	328896.751649	47.227559
3504.467855	328895.034996	47.232564
3504.326326	328899.843772	47.237569
3504.409730	328898.914055	47.242573
3504.134843	328895.418650	47.247578
3504.080467	328871.469839	47.252583
3504.123047	328865.632885	47.257588
3503.964599	328871.513638	47.262593
3504.227669	328857.851207	47.267597
3504.173462	328872.066209	47.272602
3504.039881	328867.351865	47.277607
3504.182899	328861.753627	47.282612
3504.246312	328868.439470	47.287617
3504.511697	328866.386222	47.292621
3504.224929	328866.406110	47.297626
3504.309826	328870.771739	47.302631
3504.476355	328870.490827	47.307636
3504.139614	328873.166407	47.312641
3503.975657	328865.350802	47.317645
3504.161284	328866.365307	47.322650
3504.204179	328858.160565	47.327655
3504.459246	328842.768148	47.332660
3504.190311	328849.150102	47.337665
3504.168390	328840.268198	47.342669
3504.097493	328848.910203	47.347674
3504.104796	328863.140941	47.352679
3504.409763	328848.351665	47.357684
3504.257135	328842.265515	47.362689
3504.282315	328842.006950	47.367693
3504.857486	328842.323382	47.372698
3504.330168	328831.433695	47.377703
3504.331927	328813.128010	47.382708
3504.256291	328811.943380	47.387713
3504.333034	328814.808188	47.392717
3504.174905	328820.205163	47.397722
3504.027550	328818.726357	47.402727
3504.203027	328806.147066	47.407732
3503.964887	328820.034723	47.412737
3504.104216	328821.285684	47.417741
3504.130189	328824.234896	47.422746
3504.194892	328815.110158	47.427751
3504.169193	328816.361750	47.432756
3504.119804	328826.426092	47.437761
3504.031616	328812.768266	47.442765
3503.963549	328806.414149	47.447770
3503.870948	328820.227878	47.452775
3504.353478	328815.416126	47.457780
3504.321489	328802.895093	47.462785
3504.162413	328791.463451	47.467789
3504.051538	328785.727130	47.472794
3504.012879	328792.760092	47.477799
3504.181752	328787.666952	47.482804
3504.091432	328784.167822	47.487809
3504.452506	328781.361116	47.492813
3504.263809	328792.134894	47.497818
3504.127626	328798.292189	47.502823
3504.662038	328796.120028	47.507828
3504.052069	328805.280075	47.512833
3504.309010	328797.754354	47.517837
3504.101034	328794.910315	47.522842
3504.081170	328779.765027	47.527847
3504.257141	328755.728844	47.532852
3504.077315	328760.620063	47.537857
3504.284054	328752.949517	47.542861
3504.394083	328758.915133	47.547866
3504.190291	328766.737991	47.552871
3504.353421	328757.750443	47.557876
3504.353471	328762.816900	47.562881
3504.398856	328757.768741	47.567885
3504.420633	328751.960526	47.572890
3504.428330	328754.887171	47.577895
3504.509896	328738.478320	47.582900
3503.956476	328743.835956	47.587905
3504.344097	328727.887909	47.592909
3504.607416	328726.446013	47.597914
3504.083772	328735.185067	47.602919
3504.384162	328730.478484	47.607924
3504.066049	328737.682929	47.612929
3504.199203	328732.544514	47.617933
3504.498450	328717.603359	47.622938
3504.426733	328700.404026	47.627943
3504.568518	328690.376001	47.632948
3504.306206	328693.650851	47.637953
3504.268670	328694.573342	47.642957
3504.139484	328696.426867	47.647962
3503.958831	328700.681730	47.652967
3504.380162	328706.088943	47.657972
3504.330702	328699.884633	47.662977
3504.307569	328688.431484	47.667981
3503.897414	328673.857070	47.672986
3503.898886	328670.470721	47.677991
3504.051344	328665.685683	47.682996
3503.784542	328673.874947	47.688001
3503.953749	328675.834056	47.693005
3504.141175	328681.049113	47.698010
3504.026596	328677.146460	47.703015
3504.327948	328670.352034	47.708020
3503.993735	328666.051291	47.713025
3504.207277	328670.116537	47.718029
3503.875988	328670.830873	47.723034
3503.998027	328678.754985	47.728039
3504.257680	328673.418350	47.733044
3504.065351	328682.766980	47.738049
3504.302195	328674.200581	47.743053
3504.127590	328676.850535	47.748058
3504.175201	328681.654883	47.753063
3504.271004	328683.982031	47.758068
3503.979700	328688.356227	47.763073
3503.965398	328679.269423	47.768077
3504.406311	328680.829142	47.773082
3504.164577	328678.117733	47.778087
3504.588018	328676.548683	47.783092
3504.179754	328684.302037	47.788097
3504.421006	328653.941522	47.793101
3504.117568	328650.246942	47.798106
3503.917279	328656.541681	47.803111
3504.200211	328644.276350	47.808116
3504.123358	328641.156979	47.813121
3504.052398	328646.743863	47.818125
3504.017394	328661.465060	47.823130
3503.769421	328659.391128	47.828135
3504.172699	328649.321757	47.833140
3503.938309	328661.935869	47.838145
3503.966644	328660.047389	47.843149
3503.866255	328655.429623	47.848154
3503.903871	328662.781513	47.853159
3503.804765	328662.517136	47.858164
3504.164520	328660.448963	47.863169
3504.342681	328656.398190	47.868173
3504.213901	328664.565634	47.873178
3504.225028	328657.256979	47.878183
3504.752471	328650.528646	47.883188
3504.664984	328665.410898	47.888193
3504.622313	328651.440331	47.893197
3504.247071	328647.578887	47.898202
3504.366478	328636.816064	47.903207
3504.301421	328635.349703	47.908212
3503.947806	328632.732359	47.913217
3504.292231	328637.515244	47.918221
3504.320967	328640.056673	47.923226
3504.177114	328639.570234	47.928231
3504.557547	328636.404028	47.933236
3504.171810	328637.738003	47.938241
3504.139629	328607.242480	47.943245
3504.103321	328601.265219	47.948250
3504.094889	328592.101098	47.953255
3504.318378	328586.133683	47.958260
3503.901869	328603.232032	47.963265
3504.330541	328590.587217	47.968269
3504.425720	328601.417981	47.973274
3503.915897	328595.515581	47.978279
3504.317212	328592.829804	47.983284
3504.097112	328607.096542	47.988289
3503.936643	328592.737234	47.993293
3504.141498	328590.438951	47.998298
3504.166595	328602.273721	48.003303
3504.407323	328609.237070	48.008308
3504.227494	328609.723784	48.013313
3504.513914	328590.914770	48.018317
3504.208374	328580.957451	48.023322
3503.567458	328578.436446	48.028327
3504.299974	328561.415452	48.033332
3503.705589	328572.788051	48.038337
3504.118259	328568.012788	48.043341
3504.238305	328568.248416	48.048346
3504.027436	328567.899870	48.053351
3503.938627	328567.150132	48.058356
3503.782507	328570.764634	48.063361
3503.932909	328572.242985	48.068365
3504.145158	328573.227825	48.073370
3503.754431	328582.124101	48.078375
3504.199599	328593.612404	48.083380
3504.019867	328594.582836	48.088385
3503.830269	328586.567579	48.093389
3504.190588	328591.831687	48.098394
3504.296428	328604.773914	48.103399
3504.185419	328587.275253	48.108404
3504.161322	328594.916961	48.113409
3503.839507	328584.427564	48.118413
3504.348813	328574.315961	48.123418
3504.532923	328578.258568	48.128423
3504.476456	328580.151518	48.133428
3504.172146	328584.705994	48.138433
3504.474889	328590.921211	48.143437
3504.293897	328591.280811	48.148442
3503.942628	328566.844190	48.153447
3503.936752	328589.707880	48.158452
3503.913656	328592.053827	48.163457
3504.191357	328588.343749	48.168461
3504.305014	328584.405008	48.173466
3503.759210	328570.666728	48.178471
3504.101392	328563.102049	48.183476
3504.174852	328562.122980	48.188481
3503.932733	328554.956191	48.193485
3504.253396	328554.803668	48.198490
3504.210711	328557.229093	48.203495
3504.584431	328545.967778	48.208500
3504.468169	328552.172863	48.213505
3504.332113	328554.358453	48.218509
3504.325881	328549.420279	48.223514
3504.061142	328564.559709	48.228519
3504.455483	328545.988219	48.233524
3504.090828	328557.579097	48.238529
3503.760614	328535.252288	48.243533
3504.032327	328541.243278	48.248538
3504.141811	328546.776182	48.253543
3504.440790	328529.721883	48.258548
3504.229993	328538.080524	48.263553
3504.269007	328533.237034	48.268557
3504.423306	328536.369647	48.273562
3503.985183	328540.868902	48.278567
3504.210948	328532.711593	48.283572
3504.366670	328536.836907	48.288577
3504.395106	328534.795651	48.293581
3504.233748	328540.676890	48.298586
3504.254414	328541.590181	48.303591
3504.366097	328510.409925	48.308596
3503.958519	328515.235327	48.313601
3503.935212	328495.227733	48.318605
3504.043533	328498.113020	48.323610
3503.935143	328510.656318	48.328615
3504.224499	328502.514413	48.333620
3504.190952	328515.656909	48.338625
3504.069544	328515.803412	48.343629
3504.237851	328508.418974	48.348634
3504.181109	328504.430790	48.353639
3504.399459	328493.652305	48.358644
3504.277474	328500.342032	48.363649
3504.248782	328511.166932	48.368653
3504.334727	328508.276415	48.373658
3504.071696	328502.564127	48.378663
3504.157252	328507.820761	48.383668
3504.238487	328524.662219	48.388673
3504.383137	328511.553100	48.393677
3504.332621	328484.904835	48.398682
3503.949207	328499.095573	48.403687
3504.166466	328487.451632	48.408692
3503.845705	328493.001640	48.413697
3503.830862	328492.291127	48.418701
3504.073473	328488.841188	48.423706
3503.951877	328499.349802	48.428711
3504.238129	328490.240919	48.433716
3504.166061	328497.508327	48.438721
3504.350478	328497.835617	48.443725
3504.285439	328503.268818	48.448730
3504.204797	328492.664900	48.453735
3504.388363	328488.613264	48.458740
3504.288033	328494.612156	48.463745
3504.201022	328491.137950	48.468749
3504.348567	328484.978856	48.473754
3504.162670	328475.766398	48.478759
3504.240681	328463.482516	48.483764
3503.946974	328459.531793	48.488769
3504.100444	328452.582510	48.493773
3504.009443	328451.374843	48.498778
3504.020704	328448.903485	48.503783
3504.425414	328453.040360	48.508788
3503.999179	328455.271828	48.513793
3503.838737	328449.059585	48.518797
3504.229999	328457.195753	48.523802
3504.053261	328458.038415	48.528807
3504.042725	328464.659606	48.533812
3504.422676	328468.520337	48.538817
3504.603147	328464.749245	48.543821
3504.312478	328463.751363	48.548826
3504.012598	328472.302313	48.553831
3504.124761	328463.068191	48.558836
3504.302316	328464.975066	48.563841
3504.492402	328439.077997	48.568845
3504.190903	328441.264287	48.573850
3504.285913	328428.417599	48.578855
3504.351988	328434.848463	48.583860
3504.335121	328433.425398	48.588865
3504.432727	328432.391591	48.593869
3504.315239	328440.455434	48.598874
3504.246960	328440.720836	48.603879
3504.332814	328417.182529	48.608884
3504.000072	328409.393561	48.613889
3503.843112	328399.794625	48.618893
3504.184302	328393.732208	48.623898
3503.926137	328403.320417	48.628903
3504.234875	328401.082085	48.633908
3504.093733	328405.305258	48.638913
3503.947309	328408.714557	48.643917
3504.320497	328419.043120	48.648922
3504.098614	328414.597305	48.653927
3504.408724	328401.462009	48.658932
3504.091099	328417.373620	48.663937
3503.994813	328410.947553	48.668941
3504.096942	328409.989410	48.673946
3504.204475	328406.509902	48.678951
3504.021501	328407.353551	48.683956
3504.009919	328413.669395	48.688961
3504.246588	328413.555610	48.693965
3504.243104	328412.639623	48.698970
3504.412911	328416.839096	48.703975
3504.314228	328405.856124	48.708980
3504.338852	328399.512779	48.713985
3503.891928	328390.265199	48.718989
3503.981893	328380.652682	48.723994
3503.958745	328376.149986	48.728999
3503.889299	328376.924767	48.734004
3503.892508	328391.690894	48.739009
3503.856049	328385.942778	48.744013
3504.193946	328396.837037	48.749018
3504.088722	328398.915918	48.754023
3503.871637	328388.460856	48.759028
3503.997403	328383.807319	48.764033
3503.944901	328384.732179	48.769037
3504.115370	328391.706656	48.774042
3504.183176	328407.480955	48.779047
3504.188415	328390.829500	48.784052
3503.993552	328396.461450	48.789057
3504.398752	328377.811823	48.794061
3504.198817	328390.496912	48.799066
3504.107536	328401.051666	48.804071
3504.313319	328401.757475	48.809076
3504.513263	328393.044121	48.814081
3504.051020	328396.299672	48.819085
3504.455602	328404.408280	48.824090
3504.273496	328395.118835	48.829095
3504.610221	328371.260795	48.834100
3504.266261	328364.721122	48.839105
3504.261430	328361.437595	48.844109
3504.624223	328352.876709	48.849114
3504.317886	328369.321199	48.854119
3504.801071	328351.550326	48.859124
3504.170023	328345.412475	48.864129
3504.446314	328338.800200	48.869133
3504.252677	328328.086825	48.874138
3504.517812	328318.853962	48.879143
3504.128374	328326.426158	48.884148
3504.217479	328328.194262	48.889153
3504.319962	328333.626449	48.894157
3504.681962	328336.344338	48.899162
3504.315817	328318.071240	48.904167
3504.328320	328292.304036	48.909172
3504.276338	328294.960077	48.914177
3504.396802	328287.634101	48.919181
3503.977133	328285.587302	48.924186
3503.759551	328291.630208	48.929191
3504.580207	328283.404283	48.934196
3504.201785	328299.478288	48.939201
3504.209703	328297.032914	48.944205
3504.348725	328287.412630	48.949210
3503.888479	328297.720213	48.954215
3504.430635	328286.330393	48.959220
3504.113854	328278.920785	48.964225
3503.586823	328263.193623	48.969229
3504.016493	328279.267176	48.974234
3503.761665	328294.506931	48.979239
3504.063366	328285.293743	48.984244
3503.897295	328297.056942	48.989249
3503.827640	328308.855817	48.994253
3504.369001	328301.819737	48.999258
3504.278180	328303.488988	49.004263
3504.356562	328300.090464	49.009268
3504.166151	328287.008819	49.014273
3503.963825	328270.568372	49.019277
3504.100271	328262.959810	49.024282
3503.961260	328264.585761	49.029287
3504.285550	328263.974389	49.034292
3504.274638	328276.833290	49.039297
3503.973023	328262.190719	49.044301
3504.194028	328261.875733	49.049306
3504.133353	328263.845736	49.054311
3504.165746	328269.034411	49.059316
3504.240849	328278.162593	49.064321
3504.052583	328270.019794	49.069325
3504.078764	328266.985957	49.074330
3504.365751	328271.879785	49.079335
3504.371430	328270.936888	49.084340
3504.065046	328277.375729	49.089345
3504.123099	328275.177025	49.094349
3504.586067	328259.064210	49.099354
3504.347861	328258.567226	49.104359
3504.110904	328236.021909	49.109364
3504.046928	328229.768937	49.114369
3504.168586	328230.080691	49.119373
3504.129988	328228.202782	49.124378
3503.934218	328232.689199	49.129383
3504.225520	328229.155171	49.134388
3503.972970	328239.684524	49.139393
3503.917053	328243.894233	49.144397
3504.159098	328238.152995	49.149402
3503.853389	328236.011799	49.154407
3503.908290	328242.368066	49.159412
3503.843617	328245.357091	49.164417
3503.882527	328238.782337	49.169421
3504.280775	328239.483179	49.174426
3504.182533	328241.688259	49.179431
3504.735154	328234.599474	49.184436
3504.159937	328239.604155	49.189441
3504.183366	328240.109656	49.194445
3504.566426	328239.259855	49.199450
3504.292535	328221.659563	49.204455
3504.626729	328217.380421	49.209460
3504.404697	328220.088807	49.214465
3504.468751	328215.725074	49.219469
3504.660336	328203.932391	49.224474
3503.847175	328211.087851	49.229479
3504.448730	328199.765007	49.234484
3504.258572	328183.780892	49.239489
3503.935402	328169.676366	49.244493
3504.063129	328170.241759	49.249498
3504.265814	328164.303060	49.254503
3504.477974	328156.606139	49.259508
3503.992475	328161.087445	49.264513
3504.390596	328163.239514	49.269517
3504.621011	328168.193212	49.274522
3504.198904	328169.838462	49.279527
3504.268792	328163.564321	49.284532
3504.287534	328154.166714	49.289537
3504.185121	328136.870269	49.294541
3504.400164	328144.957951	49.299546
3503.763104	328142.894598	49.304551
3503.977478	328141.918705	49.309556
3504.022791	328137.608850	49.314561
3504.114958	328136.626818	49.319565
3504.105397	328139.250698	49.324570
3503.637604	328142.099780	49.329575
3504.299280	328141.715125	49.334580
3504.084942	328142.843792	49.339585
3504.135470	328139.449665	49.344589
3504.255628	328142.664071	49.349594
3504.092559	328158.067565	49.354599
3504.380612	328150.638702	49.359604
3504.113002	328150.604642	49.364609
3504.352764	328155.251345	49.369613
3504.286448	328148.133104	49.374618
3504.237564	328154.913143	49.379623
3503.961652	328143.525336	49.384628
3504.079317	328156.185711	49.389633
3504.151413	328152.864554	49.394637
3504.416720	328140.220033	49.399642
3503.933725	328128.941342	49.404647
3504.326525	328119.000858	49.409652
3504.255145	328113.258243	49.414657
3504.106763	328118.373669	49.419661
3504.415038	328118.095805	49.424666
3504.090120	328121.125978	49.429671
3504.359868	328113.088971	49.434676
3504.262980	328123.950167	49.439681
3504.158278	328120.198683	49.444685
3504.166244	328125.238471	49.449690
3504.223336	328122.607099	49.454695
3504.182065	328127.298234	49.459700
3503.867718	328114.312533	49.464705
3504.001283	328121.776604	49.469709
3504.435889	328119.034629	49.474714
3504.015846	328106.218396	49.479719
3504.007405	328098.327206	49.484724
3504.147201	328094.460688	49.489729
3504.161430	328095.680519	49.494733
3504.294610	328098.689190	49.499738
3504.067969	328097.044686	49.504743
3504.178458	328096.645332	49.509748
3504.157207	328096.826921	49.514753
3504.213238	328100.840720	49.519757
3504.443278	328092.504471	49.524762
3504.003912	328098.887972	49.529767
3503.965623	328102.840303	49.534772
3504.367861	328101.274595	49.539777
3504.259812	328098.185593	49.544781
3504.280576	328106.507672	49.549786
3503.943665	328095.587778	49.554791
3504.144882	328085.575739	49.559796
3503.959124	328073.002518	49.564801
3503.790045	328065.391320	49.569805
3504.208355	328084.190908	49.574810
3504.056206	328090.605381	49.579815
3504.198250	328069.476765	49.584820
3503.972001	328064.089607	49.589825
3504.180673	328062.936397	49.594829
3504.005254	328063.040520	49.599834
3503.780436	328074.380224	49.604839
3503.732576	328070.161475	49.609844
3503.710766	328098.272547	49.614849
3503.584336	328110.436864	49.619853
3504.109093	328114.071042	49.624858
3503.901772	328117.795498	49.629863
3503.777504	328117.866075	49.634868
3503.838627	328114.164754	49.639873
3504.030350	328116.018478	49.644877
3504.252336	328120.515235	49.649882
3504.054929	328123.703468	49.654887
3504.324930	328112.764006	49.659892
3503.905749	328121.944890	49.664897
3503.934211	328128.050748	49.669901
3504.493811	328119.204124	49.674906
3504.044454	328124.978168	49.679911
3504.356353	328122.357431	49.684916
3504.385877	328119.297600	49.689921
3504.045406	328103.693670	49.694925
3504.388060	328078.408855	49.699930
3503.862731	328095.371761	49.704935
3504.101678	328088.027035	49.709940
3503.951731	328088.585408	49.714945
3503.778234	328094.595899	49.719949
3504.166537	328083.281292	49.724954
3504.066176	328084.290102	49.729959
3503.990984	328088.732004	49.734964
3504.237621	328089.889633	49.739969
3504.532265	328086.329611	49.744973
3504.478463	328080.405995	49.749978
3504.144136	328092.654103	49.754983
3504.004416	328088.424417	49.759988
3504.063510	328101.654177	49.764993
3503.957516	328094.822262	49.769997
3504.084764	328092.332555	49.775002
3503.745460	328095.746901	49.780007
3503.995650	328092.779482	49.785012
3503.723611	328105.756074	49.790017
3504.261314	328098.593255	49.795021
3504.394458	328097.248308	49.800026
3504.157563	328118.697451	49.805031
3504.490281	328094.610822	49.810036
3504.593470	328084.486981	49.815041
3504.537093	328068.608992	49.820045
3504.576408	328070.868710	49.825050
3504.107365	328064.272406	49.830055
3504.409869	328063.919075	49.835060
3504.020802	328070.931121	49.840065
3504.093126	328060.964916	49.845069
3504.230706	328067.384506	49.850074
3503.777672	328076.214310	49.855079
3504.091168	328078.099703	49.860084
3504.102973	328069.135999	49.865089
3504.067254	328074.233616	49.870093
3504.451413	328061.010177	49.875098
3503.924769	328056.663442	49.880103
3504.129189	328035.499496	49.885108
3504.206495	328033.730558	49.890113
3504.345143	328025.306911	49.895117
3504.328677	328018.868192	49.900122
3503.946231	328039.780252	49.905127
3504.121480	328016.838726	49.910132
3504.124124	328026.793106	49.915137
3503.897931	328030.138653	49.920141
3504.078821	328025.730978	49.925146
3503.952326	328030.435592	49.930151
3504.130795	328034.735556	49.935156
3503.880625	328037.881214	49.940161
3504.213689	328042.869611	49.945165
3504.287454	328033.870648	49.950170
3503.840648	328038.931419	49.955175
3503.992351	328039.696701	49.960180
3503.698092	328034.065695	49.965185
3503.648425	328045.810530	49.970189
3503.977559	328034.708949	49.975194
3504.081685	328035.761810	49.980199
3504.401812	328043.349153	49.985204
3504.212004	328036.912380	49.990209
3503.970107	328048.305708	49.995213
3504.278084	328030.842520	50.000218
3504.041859	328046.868637	50.005223
3504.158593	328045.195305	50.010228
3504.261729	328042.709410	50.015233
3503.954527	328047.238914	50.020237
3503.898795	328051.168546	50.025242
3504.063596	328052.873769	50.030247
3504.006398	328042.647980	50.035252
3504.087075	328058.445776	50.040257
3503.861686	328056.164577	50.045261
3504.415071	328044.136452	50.050266
3503.996789	328053.215363	50.055271
3503.892112	328050.685942	50.060276
3504.360811	328049.822600	50.065281
3504.130463	328057.573348	50.070285
3504.028264	328055.068996	50.075290
3503.762210	328060.864984	50.080295
3504.257378	328055.796589	50.085300
3504.205391	328061.609654	50.090305
3504.126074	328044.589596	50.095309
3504.326111	328034.475897	50.100314
3503.587178	328042.536191	50.105319
3504.040846	328029.174458	50.110324
3503.574830	328032.481540	50.115329
3503.835374	328059.173157	50.120333
3504.400592	328062.597262	50.125338
3504.036096	328065.760994	50.130343
3504.174885	328058.381180	50.135348
3504.334620	328054.536967	50.140353
3504.171532	328048.554247	50.145357
3504.332741	328031.139723	50.150362
3504.160389	328037.302796	50.155367
3503.973282	328032.444104	50.160372
3504.109145	328034.535800	50.165377
3504.209635	328037.320503	50.170381
3503.967423	328034.074491	50.175386
3504.088015	328034.742851	50.180391
3504.349131	328022.149893	50.185396
3504.037862	328035.361837	50.190401
3503.982441	328035.039632	50.195405
3504.242619	328040.243231	50.200410
3504.089156	328046.759755	50.205415
3504.250026	328039.936564	50.210420
3504.147812	328041.862220	50.215425
3504.360361	328037.984197	50.220429
3504.298337	328030.661588	50.225434
3504.015218	328022.635598	50.230439
3504.291361	328006.170370	50.235444
3504.191685	328004.251193	50.240449
3504.184527	328003.233943	50.245453
3504.323718	328000.284068	50.250458
3504.016655	328006.493901	50.255463
3503.919890	328002.053742	50.260468
3503.807014	328004.388441	50.265473
3503.927795	328004.140219	50.270477
3503.964464	328006.629495	50.275482
3503.807123	328006.425242	50.280487
3503.680805	328000.156648	50.285492
3503.924123	328014.528449	50.290497
3504.042556	328017.208477	50.295501
3504.292279	328004.871915	50.300506
3504.005002	328011.333218	50.305511
3504.057564	328016.824239	50.310516
3503.984592	328012.864055	50.315521
3504.085845	328018.270999	50.320525
3504.355089	328010.997856	50.325530
3503.641209	328017.628441	50.330535
3504.162577	328008.762389	50.335540
3503.953829	328009.610116	50.340545
3504.090177	328018.524967	50.345549
3504.405045	328017.074909	50.350554
3503.896533	328011.706912	50.355559
3504.136964	328022.896691	50.360564
3504.187373	328024.721839	50.365569
3504.313290	328024.880161	50.370573
3504.380531	328021.356087	50.375578
3504.184365	328030.221666	50.380583
3504.472775	328009.655470	50.385588
3504.443718	328022.924639	50.390593
3503.677770	328005.783987	50.395597
3503.954569	328007.216907	50.400602
3503.969200	328024.832797	50.405607
3504.135718	328013.858762	50.410612
3504.203648	328011.811248	50.415617
3504.133912	327999.168753	50.420621
3504.313986	327999.776791	50.425626
3503.660329	328005.226704	50.430631
3503.595082	327992.710798	50.435636
3504.079264	328013.103958	50.440641
3504.061616	328026.091264	50.445645
3504.406359	328018.424288	50.450650
3504.216547	328000.657895	50.455655
3504.260804	327999.836194	50.460660
3504.172850	328005.349431	50.465665
3504.141057	328012.686896	50.470669
3504.506565	328005.678592	50.475674
3504.040011	328004.759430	50.480679
3504.213902	328000.251021	50.485684
3504.064751	327996.455638	50.490689
3504.184160	328004.583914	50.495693
3504.382670	328003.712367	50.500698
3504.084041	327999.660559	50.505703
3504.204948	328012.447744	50.510708
3504.235676	328013.232151	50.515713
3504.063828	327980.212481	50.520717
3504.394247	327961.498198	50.525722
3503.691855	327973.397156	50.530727
3503.982082	327978.417789	50.535732
3503.913448	327960.326710	50.540737
3503.883831	327924.687627	50.545741
3503.482996	327887.808762	50.550746
3503.621410	327848.247721	50.555751
3503.558552	327786.135559	50.560756
3503.314597	327725.070374	50.565761
3503.027105	327664.470304	50.570765
3503.053496	327583.019781	50.575770
3502.459706	327509.738037	50.580775
3502.170498	327413.952343	50.585780
3501.875941	327319.975041	50.590785
3501.028900	327234.894158	50.595789
3500.716423	327128.393106	50.600794
3500.060840	327023.422843	50.605799
3500.003048	326917.110383	50.610804
3499.842809	326824.944391	50.615809
3499.041860	326692.092286	50.620813
3499.181176	326560.466163	50.625818
3498.495855	326445.774010	50.630823
3497.915576	326312.377182	50.635828
3497.644973	326187.791394	50.640833
3496.689594	326043.327225	50.645837
3496.798339	325896.301276	50.650842
3495.939622	325759.688612	50.655847
3495.312510	325600.913854	50.660852
3494.722449	325465.989543	50.665857
3493.723485	325320.843545	50.670861
3493.973390	325172.801008	50.675866
3492.772356	325030.283438	50.680871
3492.384359	324872.615201	50.685876
3491.921322	324724.735499	50.690881
3491.135505	324575.964512	50.695885
3490.764010	324413.455223	50.700890
3489.893623	324268.770811	50.705895
3489.755866	324101.004456	50.710900
3488.409162	323936.178703	50.715905
3488.134325	323781.520389	50.720909
3487.858672	323624.952332	50.725914
3486.946449	323464.970979	50.730919
3486.190210	323295.365758	50.735924
3485.646511	323138.126269	50.740929
3485.271714	322973.094067	50.745933
3484.730027	322809.666543	50.750938
3484.166243	322648.864736	50.755943
3483.622620	322461.299372	50.760948
3482.980691	322299.261659	50.765953
3481.861807	322135.083891	50.770957
3481.629533	321950.599986	50.775962
3480.795624	321801.755397	50.780967
3479.867649	321610.938958	50.785972
3479.323223	321439.106920	50.790977
3478.632470	321270.480420	50.795981
3478.007182	321112.868267	50.800986
3477.203313	320949.402355	50.805991
3476.794189	320769.679890	50.810996
3475.998594	320601.246945	50.816001
3475.277711	320438.632699	50.821005
3475.048121	320258.295207	50.826010
3474.216107	320095.315987	50.831015
3473.381179	319922.279346	50.836020
3472.762340	319743.606507	50.841025
3472.032875	319575.135756	50.846029
3471.320216	319407.655076	50.851034
3470.438342	319237.145355	50.856039
3469.986510	319066.134468	50.861044
3469.529488	318886.619600	50.866049
3468.510812	318725.067931	50.871053
3468.318629	318540.341627	50.876058
3467.357361	318384.382081	50.881063
3466.772217	318199.411694	50.886068
3466.238265	318025.661940	50.891073
3465.447228	317853.582140	50.896077
3464.839740	317684.223002	50.901082
3464.058050	317517.513790	50.906087
3463.678289	317333.680566	50.911092
3462.966831	317166.348539	50.916097
3462.095364	316995.909572	50.921101
3461.515214	316821.044599	50.926106
3460.465619	316641.593789	50.931111
3459.917330	316482.688565	50.936116
3459.019080	316311.310519	50.941121
3458.499623	316147.765898	50.946125
3458.059202	315969.618043	50.951130
3457.420391	315813.781670	50.956135
3456.917681	315627.392939	50.961140
3456.121453	315453.832920	50.966145
3455.315423	315282.540406	50.971149
3454.970684	315101.727705	50.976154
3453.839000	314942.861387	50.981159
3453.156210	314769.333207	50.986164
3452.594330	314596.447674	50.991169
3451.737132	314438.504805	50.996173
3451.204462	314266.072455	51.001178
3450.300703	314100.624643	51.006183
3449.429759	313917.575895	51.011188
3448.900435	313762.126554	51.016193
3448.223385	313610.163434	51.021197
3447.758875	313432.065974	51.026202
3447.226596	313265.997926	51.031207
3446.621522	313101.316190	51.036212
3446.039524	312927.488966	51.041217
3444.947718	312761.839654	51.046221
3444.528531	312588.750071	51.051226
3443.517104	312436.685399	51.056231
3443.277031	312261.657171	51.061236
3442.434247	312090.161640	51.066241
3441.726618	311927.302328	51.071245
3440.978470	311753.448606	51.076250
3440.315911	311574.564605	51.081255
3439.715829	311416.856814	51.086260
3438.952630	311243.794086	51.091265
3437.939942	311091.193044	51.096269
3437.859475	310914.202195	51.101274
3436.951258	310756.924187	51.106279
3436.520185	310584.266314	51.111284
3435.870700	310414.571151	51.116289
3434.784880	310263.915895	51.121293
3434.633325	310085.738191	51.126298
3433.845860	309919.909300	51.131303
3433.189459	309748.126166	51.136308
3432.500555	309589.716937	51.141313
3431.525156	309425.394034	51.146317
3430.975723	309255.223029	51.151322
3430.481394	309088.429902	51.156327
3429.801239	308922.455343	51.161332
3429.239176	308748.771469	51.166337
3428.409741	308595.603483	51.171341
3427.621849	308419.153704	51.176346
3426.676532	308260.299462	51.181351
3426.125287	308097.944916	51.186356
3425.446528	307935.559394	51.191361
3424.699901	307770.892531	51.196365
3424.697593	307605.802173	51.201370
3423.729846	307453.902460	51.206375
3422.821522	307283.734583	51.211380
3422.207789	307110.973368	51.216385
3421.483469	306959.747607	51.221389
3420.959756	306792.854224	51.226394
3420.329906	306625.646360	51.231399
3419.727754	306452.984305	51.236404
3419.142273	306300.386162	51.241409
3418.258923	306137.750618	51.246413
3417.984918	305965.774539	51.251418
3417.050039	305803.808840	51.256423
3416.204215	305634.061865	51.261428
3415.731393	305463.109743	51.266433
3414.800328	305309.240915	51.271437
3414.247956	305143.648756	51.276442
3413.823935	304976.813749	51.281447
3412.955870	304815.625754	51.286452
3412.217595	304636.540087	51.291457
3411.353812	304482.099457	51.296461
3411.189789	304322.887758	51.301466
3409.958054	304153.862111	51.306471
3409.521473	303997.901846	51.311476
3408.877290	303838.663674	51.316481
3408.202726	303678.258698	51.321485
3407.808788	303503.013446	51.326490
3406.804824	303357.736054	51.331495
3406.331140	303194.446590	51.336500
3405.908096	303028.067548	51.341505
3404.509695	302866.833907	51.346509
3404.019372	302699.191834	51.351514
3403.360247	302538.095595	51.356519
3402.549448	302382.141867	51.361524
3402.121250	302220.448518	51.366529
3401.334812	302065.356464	51.371533
3400.850031	301900.666714	51.376538
3400.273019	301751.118332	51.381543
3399.435422	301582.307573	51.386548
3398.872093	301423.996313	51.391553
3398.122976	301271.546064	51.396557
3397.804578	301100.844576	51.401562
3397.049680	300947.096147	51.406567
3396.172518	300779.742378	51.411572
3395.861028	300601.730408	51.416577
3394.605538	300448.799197	51.421581
3394.171145	300293.395078	51.426586
3393.384658	300145.380849	51.431591
3392.801951	299978.718226	51.436596
3392.377754	299818.575275	51.441601
3391.255949	299652.557847	51.446605
3390.951404	299504.950703	51.451610
3390.253575	299342.202048	51.456615
3389.504940	299168.969012	51.461620
3388.924057	299012.160750	51.466625
3388.038976	298849.976045	51.471629
3387.602318	298681.684662	51.476634
3386.985819	298529.771212	51.481639
3386.103851	298366.668769	51.486644
3385.512322	298220.353796	51.491649
3384.605119	298058.375603	51.496653
3384.334824	297897.289749	51.501658
3383.867891	297740.284081	51.506663
3382.821422	297583.573665	51.511668
3381.983235	297419.623044	51.516673
3381.695780	297259.379755	51.521677
3381.416560	297095.467788	51.526682
3380.259940	296935.794618	51.531687
3379.593654	296763.106539	51.536692
3379.150368	296608.057146	51.541697
3377.753292	296440.246682	51.546701
3377.663338	296280.913623	51.551706
3376.755803	296122.677482	51.556711
3376.330140	295967.370126	51.561716
3375.485241	295811.772411	51.566721
3374.727493	295646.203143	51.571725
3374.355506	295476.905463	51.576730
3373.524797	295335.694083	51.581735
3372.717716	295166.872432	51.586740
3372.692276	295001.034029	51.591745
3371.245070	294850.777089	51.596749
3370.799075	294685.412424	51.601754
3370.132810	294536.687128	51.606759
3369.556956	294378.702805	51.611764
3368.734915	294223.151229	51.616769
3368.129574	294062.038861	51.621773
3367.764836	293893.120784	51.626778
3366.658232	293748.462967	51.631783
3366.518948	293588.397113	51.636788
3365.658399	293423.275334	51.641793
3364.751644	293266.514055	51.646797
3364.108993	293097.792143	51.651802
3363.444917	292943.921022	51.656807
3362.857047	292789.095451	51.661812
3361.775650	292636.512569	51.666817
3361.074460	292482.901693	51.671821
3360.837706	292317.655015	51.676826
3359.841932	292174.404878	51.681831
3359.236385	292022.484910	51.686836
3359.183281	291859.577361	51.691841
3358.276951	291695.327528	51.696845
3357.796826	291547.156638	51.701850
3356.870624	291387.239241	51.706855
3356.367391	291227.534994	51.711860
3355.521285	291058.258106	51.716865
3354.633827	290912.010415	51.721869
3354.294471	290744.970739	51.726874
3353.508971	290603.418273	51.731879
3352.903919	290445.767075	51.736884
3352.356257	290273.513708	51.741889
3351.412483	290137.767207	51.746893
3350.895593	289969.227074	51.751898
3350.114717	289815.041474	51.756903
3349.512936	289643.025491	51.761908
3349.026715	289510.440733	51.766913
3347.842071	289342.744411	51.771917
3347.622207	289182.153732	51.776922
3346.873627	289031.910124	51.781927
3346.142820	288873.615793	51.786932
3345.853869	288723.350273	51.791937
3344.754140	288572.983703	51.796941
3344.361458	288407.530122	51.801946
3343.584193	288258.003777	51.806951
3342.927836	288090.732579	51.811956
3342.144507	287932.165937	51.816961
3341.348884	287779.025833	51.821965
3341.004144	287620.211399	51.826970
3340.116410	287461.966662	51.831975
3339.464107	287301.163289	51.836980
3339.092391	287160.587970	51.841985
3338.242120	286998.440498	51.846989
3337.558539	286846.046299	51.851994
3336.900702	286685.472734	51.856999
3336.258965	286536.993861	51.862004
3335.722851	286372.529769	51.867009
3334.674650	286217.824455	51.872013
3334.462114	286050.583966	51.877018
3333.520417	285899.325334	51.882023
3332.849849	285742.981083	51.887028
3332.249629	285591.388176	51.892033
3331.387912	285435.965423	51.897037
3330.872153	285275.292401	51.902042
3330.098784	285133.837548	51.907047
3329.314830	284975.091472	51.912052
3328.752605	284830.113991	51.917057
3327.714545	284673.343574	51.922061
3327.282331	284527.632324	51.927066
3326.464105	284374.927404	51.932071
3325.562910	284217.116457	51.937076
3325.167637	284071.424689	51.942081
3324.757769	283921.431064	51.947085
3324.038181	283779.687136	51.952090
3322.917628	283633.498718	51.957095
3322.708803	283468.854416	51.962100
3321.924913	283327.069596	51.967105
3320.989651	283178.788817	51.972109
3320.795297	283026.188552	51.977114
3319.979478	282879.340489	51.982119
3319.420391	282734.081746	51.987124
3319.136778	282578.362884	51.992129
3317.988637	282426.244406	51.997133
3317.386199	282277.503257	52.002138
3316.704230	282134.173921	52.007143
3316.083600	281979.043045	52.012148
3315.684835	281819.827582	52.017153
3314.780353	281678.443461	52.022157
3314.644971	281508.209436	52.027162
3313.589387	281351.135216	52.032167
3313.060401	281199.937248	52.037172
3312.330299	281040.901356	52.042177
3311.719220	280894.606224	52.047181
3310.989273	280729.687063	52.052186
3310.130547	280591.351690	52.057191
3309.620571	280430.243390	52.062196
3308.982112	280279.546458	52.067201
3307.935349	280136.223493	52.072205
3307.712511	279974.000020	52.077210
3307.134285	279829.533227	52.082215
3306.077326	279674.012471	52.087220
3305.653968	279521.931570	52.092225
3304.814109	279363.243820	52.097229
3304.514890	279216.771744	52.102234
3303.539303	279056.220761	52.107239
3302.832807	278894.837673	52.112244
3302.463300	278741.678478	52.117249
3301.729201	278594.460127	52.122253
3301.150857	278429.465670	52.127258
3300.043430	278275.659094	52.132263
3299.154055	278134.832350	52.137268
3298.880433	277982.931324	52.142273
3298.124120	277824.128302	52.147277
3297.663766	277668.411061	52.152282
3296.462312	277531.352016	52.157287
3295.871287	277377.438210	52.162292
3295.249660	277236.569046	52.167297
3294.586748	277087.199964	52.172301
3293.954063	276939.201385	52.177306
3293.519356	276804.389576	52.182311
3292.603724	276646.197449	52.187316
3292.421078	276492.932111	52.192321
3291.282619	276347.280199	52.197325
3290.898291	276188.341834	52.202330
3290.016037	276051.919883	52.207335
3289.437842	275900.627228	52.212340
3288.919808	275749.987233	52.217345
3288.284427	275598.576279	52.222349
3287.755918	275450.612121	52.227354
3286.854129	275312.385000	52.232359
3286.285395	275153.068304	52.237364
3285.673764	275002.162966	52.242369
3284.961763	274857.462327	52.247373
3284.446132	274691.897485	52.252378
3283.803686	274550.598617	52.257383
3283.100457	274394.512234	52.262388
3282.607626	274237.170094	52.267393
3281.656202	274079.263796	52.272397
3280.906192	273926.801349	52.277402
3280.458624	273777.601959	52.282407
3279.687062	273624.480762	52.287412
3279.142989	273470.610477	52.292417
3278.295033	273324.479724	52.297421
3277.829030	273165.503438	52.302426
3277.017705	273019.214106	52.307431
3276.222546	272869.815089	52.312436
3275.752869	272712.647684	52.317441
3274.567272	272565.093247	52.322445
3273.782683	272404.104501	52.327450
3273.491825	272269.626639	52.332455
3273.171026	272124.558692	52.337460
3272.279953	271978.434898	52.342465
3271.455533	271834.439921	52.347469
3270.862894	271666.824608	52.352474
3270.544554	271520.559338	52.357479
3269.537656	271380.209795	52.362484
3269.356855	271216.680747	52.367489
3268.315072	271058.789087	52.372493
3267.606673	270905.021522	52.377498
3266.987401	270760.815973	52.382503
3266.347363	270619.160566	52.387508
3265.757576	270471.155624	52.392513
3264.734389	270320.341352	52.397517
3264.245955	270167.150367	52.402522
3263.544273	270029.019444	52.407527
3262.670954	269886.280469	52.412532
3262.295894	269723.521032	52.417537
3261.628131	269583.678454	52.422541
3261.226451	269436.739098	52.427546
3260.403367	269297.124897	52.432551
3259.713754	269139.483547	52.437556
3258.752909	268984.813994	52.442561
3258.180596	268838.054579	52.447565
3257.613986	268686.429862	52.452570
3256.861327	268535.700537	52.457575
3256.057038	268390.913516	52.462580
3255.622886	268247.315922	52.467585
3254.690424	268104.382964	52.472589
3254.256357	267949.350203	52.477594
3253.271207	267812.716306	52.482599
3252.890274	267659.534403	52.487604
3252.320969	267527.750158	52.492609
3251.380647	267381.049349	52.497613
3251.042068	267230.967993	52.502618
3250.186134	267078.370775	52.507623
3249.386346	266942.548242	52.512628
3249.096132	266802.799442	52.517633
3248.108844	266656.895797	52.522637
3247.564851	266501.880880	52.527642
3247.100162	266352.430991	52.532647
3246.428962	266205.356890	52.537652
3245.810222	266052.977171	52.542657
3244.809372	265910.692390	52.547661
3244.281547	265768.918590	52.552666
3243.532649	265623.308664	52.557671
3242.914263	265477.958290	52.562676
3242.440568	265330.242017	52.567681
3241.428339	265184.495631	52.572685
3241.216630	265028.919329	52.577690
3240.522915	264883.326411	52.582695
3239.752319	264733.543487	52.587700
3239.330320	264589.232033	52.592705
3238.195246	264433.547374	52.597709
3237.932400	264287.580907	52.602714
3236.748657	264144.689007	52.607719
3236.213528	263990.157557	52.612724
3235.983884	263847.318579	52.617729
3234.744783	263698.450646	52.622733
3234.328448	263551.872067	52.627738
3233.559801	263409.882581	52.632743
3232.976874	263267.456287	52.637748
3232.462122	263122.930899	52.642753
3231.712219	262983.358082	52.647757
3231.168735	262822.665256	52.652762
3230.633016	262687.923049	52.657767
3229.948595	262534.001654	52.662772
3229.078332	262378.836343	52.667777
3228.315859	262240.742978	52.672781
3227.741889	262080.386438	52.677786
3226.998902	261929.123265	52.682791
3226.212699	261786.780737	52.687796
3226.021052	261653.028730	52.692801
3224.797628	261514.499271	52.697805
3224.415828	261358.391306	52.702810
3223.686697	261207.533798	52.707815
3222.813690	261077.964695	52.712820
3222.161926	260931.195401	52.717825
3221.373726	260789.413973	52.722829
3221.028702	260639.820323	52.727834
3220.107102	260515.403647	52.732839
3218.884655	260374.225959	52.737844
3218.645520	260222.578372	52.742849
3218.150450	260106.778876	52.747853
3217.679969	259952.468474	52.752858
3216.915831	259811.982606	52.757863
3216.081923	259669.750588	52.762868
3215.904436	259522.117535	52.767873
3215.059826	259388.571816	52.772877
3214.379800	259231.901047	52.777882
3213.541535	259100.697493	52.782887
3212.999231	258955.949390	52.787892
3212.470632	258799.866158	52.792897
3211.849816	258671.022377	52.797901
3211.062522	258516.661112	52.802906
3210.208501	258385.485904	52.807911
3209.630240	258227.373503	52.812916
3209.199144	258093.253722	52.817921
3208.291849	257946.042699	52.822925
3207.898164	257793.580625	52.827930
3207.247917	257667.263324	52.832935
3206.359709	257513.147896	52.837940
3205.662871	257366.948111	52.842945
3205.137043	257218.658511	52.847949
3204.251860	257085.120514	52.852954
3203.626603	256925.997758	52.857959
3203.269115	256801.035330	52.862964
3202.433424	256651.598175	52.867969
3201.382689	256521.346529	52.872973
3201.191153	256355.457679	52.877978
3200.285934	256228.442997	52.882983
3199.590321	256090.495260	52.887988
3198.866199	255944.224351	52.892993
3198.056076	255811.388356	52.897997
3197.565025	255676.439122	52.903002
3197.172764	255526.907140	52.908007
3196.486993	255382.871672	52.913012
3195.551754	255241.702626	52.918017
3194.906427	255106.778181	52.923021
3194.457663	254958.045040	52.928026
3193.501394	254819.859268	52.933031
3192.598411	254684.517471	52.938036
3192.301569	254533.697784	52.943041
3191.524872	254404.320949	52.948045
3190.858885	254264.918161	52.953050
3189.876566	254119.122383	52.958055
3189.518107	253983.134649	52.963060
3188.942472	253861.417387	52.968065
3188.355062	253714.820897	52.973069
3187.543351	253580.102115	52.978074
3186.818854	253437.653169	52.983079
3186.207548	253302.775546	52.988084
3185.569175	253158.021174	52.993089
3184.796864	253025.206577	52.998093
3184.086569	252888.282111	53.003098
3183.652740	252745.889583	53.008103
3182.957035	252618.283854	53.013108
3182.532777	252482.129377	53.018113
3181.859718	252337.814090	53.023117
3181.049933	252198.359226	53.028122
3180.711061	252062.267964	53.033127
3179.698961	251924.653466	53.038132
3179.173444	251781.104761	53.043137
3178.306902	251637.202670	53.048141
3177.573861	251507.158869	53.053146
3177.290333	251361.993299	53.058151
3176.191416	251225.284433	53.063156
3175.922389	251078.257755	53.068161
3174.966501	250945.371932	53.073165
3174.559634	250798.621977	53.078170
3173.814982	250669.242794	53.083175
3173.155443	250520.852280	53.088180
3172.650556	250375.620733	53.093185
3171.534622	250230.205872	53.098189
3171.469348	250098.020208	53.103194
3170.268429	249960.768278	53.108199
3169.716837	249820.357764	53.113204
3169.297045	249670.605851	53.118209
3167.938429	249544.278815	53.123213
3167.575144	249405.035790	53.128218
3166.945306	249270.750050	53.133223
3166.340923	249150.670550	53.138228
3165.827133	248991.333397	53.143233
3164.933489	248862.259394	53.148237
3164.216425	248725.721443	53.153242
3163.714037	248602.519363	53.158247
3163.228753	248449.010010	53.163252
3162.876534	248305.589791	53.168257
3161.773884	248164.682263	53.173261
3161.426926	248013.927268	53.178266
3160.424055	247882.044661	53.183271
3159.567448	247740.258227	53.188276
3159.163478	247611.820867	53.193281
3158.018844	247481.183419	53.198285
3157.831251	247328.315704	53.203290
3157.155216	247208.198173	53.208295
3156.549936	247065.685049	53.213300
3155.679797	246930.624537	53.218305
3154.786091	246796.102665	53.223309
3154.347613	246655.906412	53.228314
3153.879206	246513.321252	53.233319
3153.229629	246387.699623	53.238324
3152.826281	246245.792015	53.243329
3151.761608	246109.668049	53.248333
3151.192001	245970.308135	53.253338
3150.781014	245828.682285	53.258343
3149.664336	245680.929175	53.263348
3149.114466	245549.995683	53.268353
3148.172934	245415.151665	53.273357
3147.296651	245289.490517	53.278362
3146.797312	245152.361288	53.283367
3146.181994	245021.998905	53.288372
3145.460650	244877.672889	53.293377
3144.678622	244756.835764	53.298381
3144.000365	244620.728546	53.303386
3143.415825	244499.656682	53.308391
3142.910384	244362.376442	53.313396
3142.459273	244234.484458	53.318401
3141.696576	244110.767286	53.323405
3140.955321	243963.364123	53.328410
3140.408282	243824.435790	53.333415
3139.802431	243697.994877	53.338420
3139.414353	243567.572521	53.343425
3138.357672	243431.450039	53.348429
3137.764578	243294.490390	53.353434
3137.190410	243166.542547	53.358439
3136.513355	243034.332980	53.363444
3136.254813	242891.056414	53.368449
3135.537433	242760.916187	53.373453
3134.358849	242608.567192	53.378458
3133.842978	242475.848876	53.383463
3132.939919	242344.439756	53.388468
3132.445270	242197.789050	53.393473
3131.635908	242083.325025	53.398477
3131.189368	241946.063558	53.403482
3130.237509	241803.840172	53.408487
3129.806491	241670.701866	53.413492
3129.288943	241536.787991	53.418497
3128.294292	241408.552013	53.423501
3127.911515	241273.929557	53.428506
3127.035249	241138.417688	53.433511
3126.486504	241004.687601	53.438516
3125.868307	240866.919777	53.443521
3125.058945	240740.590515	53.448525
3124.491124	240608.773743	53.453530
3123.744343	240473.675047	53.458535
3123.007071	240354.948698	53.463540
3122.580212	240204.877473	53.468545
3121.737401	240087.186680	53.473549
3121.372890	239951.926242	53.478554
3120.685421	239820.562198	53.483559
3119.867495	239689.677310	53.488564
3119.381906	239531.900552	53.493569
3118.782621	239400.701289	53.498573
3117.777991	239259.457002	53.503578
3117.200189	239133.398438	53.508583
3116.721883	239004.166705	53.513588
3116.084305	238864.443612	53.518593
3115.014766	238725.502051	53.523597
3114.236273	238588.933699	53.528602
3113.827344	238465.752078	53.533607
3113.167784	238334.869179	53.538612
3112.686021	238206.504704	53.543617
3111.600220	238085.340432	53.548621
3111.067941	237926.147360	53.553626
3110.580355	237800.967282	53.558631
3109.960132	237676.444938	53.563636
3109.414437	237533.194984	53.568641
3108.775350	237409.006966	53.573645
3107.958295	237269.390713	53.578650
3107.454119	237128.553794	53.583655
3106.736428	236994.753385	53.588660
3106.044448	236870.981787	53.593665
3104.920305	236744.579574	53.598669
3104.804127	236602.357840	53.603674
3103.982691	236466.282793	53.608679
3103.207549	236339.189247	53.613684
3102.770115	236198.979601	53.618689
3101.728949	236073.736395	53.623693
3100.955183	235942.696270	53.628698
3100.553231	235810.273369	53.633703
3099.775142	235685.167246	53.638708
3099.380237	235542.074395	53.643713
3098.420790	235419.263543	53.648717
3097.725191	235282.839121	53.653722
3097.198580	235158.483211	53.658727
3096.443274	235027.772364	53.663732
3096.030758	234897.567628	53.668737
3094.992349	234765.094038	53.673741
3094.195385	234630.341653	53.678746
3093.990928	234499.467928	53.683751
3093.058123	234380.931938	53.688756
3092.874315	234236.356140	53.693761
3091.932434	234117.770975	53.698765
3091.013888	233989.582706	53.703770
3090.557510	233850.525159	53.708775
3089.761148	233731.229933	53.713780
3089.077326	233593.991153	53.718785
3088.513382	233472.265947	53.723789
3087.862388	233342.432025	53.728794
3087.102940	233212.437202	53.733799
3086.822227	233087.255640	53.738804
3086.091688	232954.277446	53.743809
3085.413816	232825.008656	53.748813
3084.685775	232698.930815	53.753818
3083.878717	232553.208494	53.758823
3083.301828	232430.417229	53.763828
3082.722225	232292.909193	53.768833
3081.962351	232174.908720	53.773837
3081.159110	232039.753537	53.778842
3081.083836	231909.066579	53.783847
3080.001760	231778.284523	53.788852
3079.480766	231635.497453	53.793857
3078.549170	231523.457717	53.798861
3078.038606	231388.104385	53.803866
3077.481864	231253.038645	53.808871
3076.542458	231130.255543	53.813876
3076.030990	230995.030242	53.818881
3075.145998	230864.523836	53.823885
3074.688999	230727.762581	53.828890
3074.284499	230606.881569	53.833895
3073.226570	230477.268801	53.838900
3072.932128	230340.304167	53.843905
3071.709414	230223.092388	53.848909
3071.178958	230084.026691	53.853914
3070.397427	229956.891660	53.858919
3069.469984	229834.897741	53.863924
3068.983435	229702.140234	53.868929
3068.225717	229586.026941	53.873933
3067.891507	229458.490820	53.878938
3067.153725	229339.803056	53.883943
3066.447188	229210.187436	53.888948
3066.052223	229077.416371	53.893953
3065.314766	228955.113519	53.898957
3064.804559	228828.726477	53.903962
3064.312460	228692.483132	53.908967
3063.366826	228569.246231	53.913972
3062.546612	228434.888451	53.918977
3061.735033	228311.936236	53.923981
3061.383478	228174.933078	53.928986
3060.531899	228059.244054	53.933991
3059.869600	227929.827034	53.938996
3059.529702	227794.630392	53.944001
3058.465628	227676.403928	53.949005
3058.023672	227554.616438	53.954010
3057.217681	227420.105231	53.959015
3056.736951	227299.953758	53.964020
3056.038421	227165.833325	53.969025
3055.201176	227056.101294	53.974029
3054.815762	226915.197250	53.979034
3054.274246	226782.338359	53.984039
3053.237069	226669.875963	53.989044
3052.983585	226534.336669	53.994049
3051.889341	226406.046981	53.999053
3051.150391	226272.329022	54.004058
3050.810831	226142.940050	54.009063
3049.961186	226019.411606	54.014068
3049.412094	225895.555707	54.019073
3048.669056	225783.748131	54.024077
3048.060017	225649.679633	54.029082
3047.501901	225526.958718	54.034087
3046.712680	225397.272916	54.039092
3046.140181	225262.460915	54.044097
3045.372747	225138.691647	54.049101
3044.870840	225007.395172	54.054106
3044.046937	224893.883041	54.059111
3043.523202	224763.659756	54.064116
3042.740309	224630.702528	54.069121
3042.134321	224507.748866	54.074125
3041.634204	224372.506805	54.079130
3041.006028	224251.173775	54.084135
3040.314422	224115.491447	54.089140
3039.979179	223992.164745	54.094145
3039.016897	223864.940256	54.099149
3038.174087	223734.947378	54.104154
3037.596716	223608.209769	54.109159
3036.554808	223471.120048	54.114164
3035.865061	223335.171440	54.119169
3035.425218	223219.729615	54.124173
3034.533589	223086.550331	54.129178
3033.908841	222957.568083	54.134183
3033.232865	222847.217952	54.139188
3032.977182	222710.068774	54.144193
3031.960493	222593.191607	54.149197
3031.355576	222468.700665	54.154202
3030.574935	222340.609752	54.159207
3030.168019	222224.260387	54.164212
3029.384294	222094.579153	54.169217
3028.486866	221975.901888	54.174221
3027.709053	221846.691140	54.179226
3027.137660	221731.055967	54.184231
3026.243635	221616.032145	54.189236
3025.897687	221485.773470	54.194241
3025.328962	221375.523057	54.199245
3024.423584	221248.853990	54.204250
3024.067605	221136.940863	54.209255
3023.438274	221013.105383	54.214260
3022.519176	220899.716012	54.219265
3021.884509	220777.702092	54.224269
3021.424562	220644.484216	54.229274
3020.971277	220525.649832	54.234279
3019.773651	220395.667893	54.239284
3019.561610	220271.513007	54.244289
3018.760941	220153.803482	54.249293
3018.276782	220020.896068	54.254298
3017.383356	219898.160796	54.259303
3016.843922	219785.005813	54.264308
3016.490709	219640.074586	54.269313
3015.436363	219534.651823	54.274317
3014.791509	219404.915104	54.279322
3014.104247	219289.238435	54.284327
3013.200504	219151.434611	54.289332
3012.764251	219041.981389	54.294337
3012.256076	218915.380759	54.299341
3011.529428	218779.713575	54.304346
3010.936606	218676.586635	54.309351
3009.936394	218547.569626	54.314356
3009.566817	218412.406697	54.319361
3008.768721	218292.153969	54.324365
3007.908159	218178.084931	54.329370
3007.193533	218045.574047	54.334375
3006.841656	217938.196722	54.339380
3006.316225	217818.958144	54.344385
3005.684728	217694.784984	54.349389
3004.853686	217566.137579	54.354394
3004.227737	217445.489902	54.359399
3003.152845	217329.317703	54.364404
3002.765562	217205.959586	54.369409
3002.223757	217085.833822	54.374413
3001.519583	216972.047477	54.379418
3000.991031	216846.281149	54.384423
3000.246064	216712.122840	54.389428
2999.820540	216591.508558	54.394433
2998.813990	216459.683327	54.399437
2998.405720	216334.268023	54.404442
2997.581017	216223.696899	54.409447
2996.818378	216108.190127	54.414452
2996.531154	215975.055459	54.419457
2995.841942	215859.982985	54.424461
2994.894730	215722.370975	54.429466
2994.253739	215597.617561	54.434471
2993.586956	215481.205674	54.439476
2992.763992	215366.167937	54.444481
2991.997349	215239.207577	54.449485
2991.448226	215122.090341	54.454490
2990.897469	215003.687990	54.459495
2990.045256	214886.568230	54.464500
2989.760978	214759.036005	54.469505
2988.588766	214649.349809	54.474509
2988.313318	214533.539487	54.479514
2987.977321	214405.328790	54.484519
2987.204553	214282.049710	54.489524
2986.504171	214156.379203	54.494529
2985.700756	214029.987003	54.499533
2985.293998	213903.608622	54.504538
2984.641145	213779.967829	54.509543
2983.958972	213664.999831	54.514548
2983.249632	213539.128264	54.519553
2982.457244	213419.901466	54.524557
2981.540717	213282.378723	54.529562
2981.072935	213151.874796	54.534567
2980.148932	213040.751887	54.539572
2979.724792	212925.057022	54.544577
2978.965617	212794.434475	54.549581
2978.414479	212678.581960	54.554586
2977.749319	212551.063389	54.559591
2976.946581	212438.789520	54.564596
2976.826058	212305.966736	54.569601
2976.026266	212177.948369	54.574605
2975.370402	212062.711751	54.579610
2974.529351	211924.454451	54.584615
2973.656955	211807.979782	54.589620
2972.805361	211676.304993	54.594625
2972.080470	211557.160040	54.599629
2971.714848	211443.176828	54.604634
2970.917946	211322.121819	54.609639
2970.200381	211208.831132	54.614644
2969.865328	211088.059831	54.619649
2969.295221	210964.004044	54.624653
2968.223762	210835.560460	54.629658
2967.844034	210715.369689	54.634663
2967.071447	210600.166932	54.639668
2966.503094	210474.100870	54.644673
2965.602123	210350.200495	54.649677
2965.248523	210239.361265	54.654682
2964.416233	210111.772230	54.659687
2963.658489	209999.202828	54.664692
2962.861553	209866.988616	54.669697
2962.317852	209748.136596	54.674701
2961.548262	209634.716992	54.679706
2960.905187	209522.804856	54.684711
2960.298405	209395.423415	54.689716
2959.562438	209286.275527	54.694721
2958.897864	209170.574684	54.699725
2958.152124	209044.259610	54.704730
2957.638733	208929.693471	54.709735
2956.869925	208811.998897	54.714740
2956.212548	208696.705082	54.719745
2955.681043	208575.727952	54.724749
2954.762272	208456.339634	54.729754
2954.517507	208342.470247	54.734759
2953.513414	208228.810378	54.739764
2952.710776	208110.982520	54.744769
2952.069531	207995.114764	54.749773
2951.516071	207887.989550	54.754778
2951.468912	207760.726562	54.759783
2950.123886	207650.634422	54.764788
2950.054762	207523.413595	54.769793
2949.188162	207411.591642	54.774797
2948.361825	207288.322011	54.779802
2947.691636	207171.187736	54.784807
2946.949463	207059.015846	54.789812
2946.394222	206939.572989	54.794817
2945.587035	206824.319209	54.799821
2945.203850	206700.077031	54.804826
2944.713440	206591.544213	54.809831
2943.791283	206471.765860	54.814836
2943.268207	206335.596172	54.819841
2942.764083	206222.140961	54.824845
2941.954906	206094.887639	54.829850
2941.370359	205978.493043	54.834855
2940.523946	205858.754855	54.839860
2939.825598	205745.471309	54.844865
2938.875456	205621.741151	54.849869
2938.421839	205518.333302	54.854874
2938.211331	205395.262843	54.859879
2937.040142	205274.724599	54.864884
2936.564425	205153.389266	54.869889
2936.064891	205035.532277	54.874893
2935.364341	204911.827749	54.879898
2934.677317	204798.989684	54.884903
2933.720513	204674.753549	54.889908
2933.354358	204553.618479	54.894913
2932.691049	204436.221342	54.899917
2932.259607	204313.048180	54.904922
2931.603236	204194.555980	54.909927
2930.478975	204067.598805	54.914932
2930.031028	203949.379544	54.919937
2929.146367	203830.020686	54.924941
2928.520952	203708.546671	54.929946
2928.134864	203590.674695	54.934951
2927.214396	203479.186991	54.939956
2926.600863	203356.655583	54.944961
2925.857556	203248.907202	54.949965
2925.281847	203121.750761	54.954970
2924.874097	203002.229061	54.959975
2923.811529	202880.966027	54.964980
2923.307049	202761.281992	54.969985
2922.975065	202646.114052	54.974989
2921.981787	202529.625752	54.979994
2921.447000	202408.216551	54.984999
2920.745432	202286.185005	54.990004
2920.194443	202169.894672	54.995009
2919.171534	202054.442850	55.000013
2918.110008	201937.317584	55.005018
2917.767920	201817.418981	55.010023
2916.865611	201713.020156	55.015028
2916.415508	201601.283570	55.020033
2915.692758	201488.190560	55.025037
2915.084493	201381.595172	55.030042
2914.613320	201262.290867	55.035047
2913.926250	201154.092249	55.040052
2913.555627	201027.913453	55.045057
2912.765336	200913.725200	55.050061
2912.148259	200797.931799	55.055066
2911.460030	200671.447802	55.060071
2910.543126	200557.254892	55.065076
2910.058216	200441.237718	55.070081
2909.191888	200315.011807	55.075085
2908.843970	200201.480353	55.080090
2907.801384	200094.040029	55.085095
2907.214921	199984.568003	55.090100
2906.776713	199861.762095	55.095105
2905.785022	199756.859439	55.100109
2905.093032	199634.246937	55.105114
2904.485700	199514.408126	55.110119
2903.953760	199413.887159	55.115124
2903.533740	199298.027599	55.120129
2902.894543	199178.830841	55.125133
2902.118514	199061.946529	55.130138
2901.307653	198947.689350	55.135143
2900.456055	198826.198329	55.140148
2899.954414	198703.621451	55.145153
2899.303750	198586.781960	55.150157
2898.699813	198480.026202	55.155162
2897.970678	198369.243961	55.160167
2897.130866	198247.485181	55.165172
2896.797289	198145.510020	55.170177
2896.049597	198018.978086	55.175181
2895.525055	197906.052104	55.180186
2894.799265	197785.841489	55.185191
2893.890727	197679.224661	55.190196
2893.649925	197557.690751	55.195201
2892.651394	197445.756994	55.200205
2891.707540	197330.608207	55.205210
2891.299323	197206.963880	55.210215
2890.584689	197105.623692	55.215220
2889.666721	196984.503735	55.220225
2889.269471	196879.359984	55.225229
2888.988965	196769.731654	55.230234
2888.172176	196643.901125	55.235239
2887.157324	196539.835645	55.240244
2886.558166	196419.035541	55.245249
2885.888143	196312.205614	55.250253
2885.188256	196202.988456	55.255258
2885.015215	196088.522018	55.260263
2883.837594	195981.620464	55.265268
2883.251876	195862.422807	55.270273
2882.651992	195755.290277	55.275277
2882.045495	195640.002780	55.280282
2881.484754	195518.078984	55.285287
2880.848165	195413.917725	55.290292
2880.508544	195287.951349	55.295297
2879.712306	195186.233426	55.300301
2878.988723	195074.108613	55.305306
2878.537040	194944.305434	55.310311
2877.795666	194823.417113	55.315316
2877.093641	194698.705649	55.320321
2876.292543	194587.459423	55.325325
2875.219640	194473.711695	55.330330
2874.730315	194347.058830	55.335335
2874.039615	194251.598973	55.340340
2873.431255	194132.307186	55.345345
2872.701923	194020.172909	55.350349
2871.966937	193914.732501	55.355354
2871.508528	193790.150131	55.360359
2870.719717	193695.444853	55.365364
2870.171919	193568.408785	55.370369
2869.165408	193473.865640	55.375373
2868.534007	193348.153915	55.380378
2868.207726	193235.881241	55.385383
2867.352745	193128.642024	55.390388
2866.745125	193011.414034	55.395393
2865.889479	192899.556764	55.400397
2865.424208	192797.943980	55.405402
2864.764025	192691.425555	55.410407
2863.979413	192578.514440	55.415412
2863.488295	192467.185709	55.420417
2862.396999	192360.163718	55.425421
2861.922209	192246.669924	55.430426
2861.722016	192128.908757	55.435431
2860.470799	192031.684342	55.440436
2860.013188	191929.779509	55.445441
2859.472154	191815.762829	55.450445
2859.271671	191707.850532	55.455450
2858.495134	191581.504710	55.460455
2857.372307	191477.823133	55.465460
2856.870511	191359.526324	55.470465
2855.928629	191244.938305	55.475469
2855.378919	191136.573659	55.480474
2854.962978	191023.582326	55.485479
2853.993227	190926.799036	55.490484
2853.591836	190808.691246	55.495489
2852.861557	190696.920974	55.500493
2852.282008	190578.638395	55.505498
2851.548902	190472.416296	55.510503
2850.846150	190368.467022	55.515508
2850.205687	190256.632664	55.520513
2849.467034	190139.406918	55.525517
2848.986493	190035.334121	55.530522
2848.464682	189914.830276	55.535527
2847.786230	189816.705383	55.540532
2846.863432	189691.481856	55.545537
2846.017707	189585.483134	55.550541
2845.503566	189477.192954	55.555546
2844.896524	189374.299400	55.560551
2844.158671	189264.683815	55.565556
2843.858880	189144.973736	55.570561
2843.333896	189030.566749	55.575565
2842.341701	188916.539368	55.580570
2842.047734	188804.933461	55.585575
2840.916991	188699.681604	55.590580
2840.488129	188578.148655	55.595585
2839.495218	188472.760980	55.600589
2838.895580	188359.321630	55.605594
2838.353838	188245.898832	55.610599
2837.663814	188139.700604	55.615604
2837.067688	188025.968896	55.620609
2836.357715	187917.420718	55.625613
2835.507284	187809.263981	55.630618
2834.959207	187695.436418	55.635623
2834.057072	187579.782330	55.640628
2833.556828	187474.955003	55.645633
2833.034583	187368.999133	55.650637
2832.184504	187251.569255	55.655642
2831.622697	187144.157132	55.660647
2830.627740	187047.614819	55.665652
2829.798058	186936.276347	55.670657
2829.560137	186836.930254	55.675661
2828.840711	186733.373353	55.680666
2828.374578	186615.744355	55.685671
2827.543009	186506.035625	55.690676
2826.867522	186397.956274	55.695681
2826.225826	186301.970234	55.700685
2825.665250	186191.481480	55.705690
2825.093701	186077.572591	55.710695
2824.096671	185967.331606	55.715700
2823.768970	185858.040784	55.720705
2823.020234	185748.816905	55.725709
2822.385759	185648.187712	55.730714
2821.367128	185528.728061	55.735719
2820.818841	185436.621856	55.740724
2820.301970	185333.888405	55.745729
2819.397141	185226.865886	55.750733
2818.508140	185114.040136	55.755738
2818.150349	185007.758395	55.760743
2817.640254	184923.598074	55.765748
2817.442732	184805.689524	55.770753
2816.508509	184701.255347	55.775757
2815.100682	184598.893664	55.780762
2814.780603	184492.505401	55.785767
2814.222646	184395.047210	55.790772
2813.778355	184273.235559	55.795777
2813.061605	184170.778132	55.800781
2812.130896	184065.454404	55.805786
2811.941229	183951.325043	55.810791
2810.794511	183851.264412	55.815796
2810.461395	183747.106183	55.820801
2809.623113	183647.124374	55.825805
2809.151797	183532.455529	55.830810
2808.713136	183422.819310	55.835815
2807.605900	183324.381901	55.840820
2807.125830	183204.194410	55.845825
2806.592031	183100.260302	55.850829
2805.959524	182988.633244	55.855834
2805.429381	182878.542196	55.860839
2804.584904	182776.095509	55.865844
2803.815567	182658.168739	55.870849
2803.043557	182546.806594	55.875853
2802.224010	182442.321427	55.880858
2801.717375	182334.225170	55.885863
2800.562667	182230.124330	55.890868
2800.205485	182128.645074	55.895873
2799.665019	182028.594344	55.900877
2799.152434	181929.531630	55.905882
2798.457669	181815.818541	55.910887
2797.410513	181717.324355	55.915892
2796.857648	181607.888855	55.920897
2796.305824	181506.276515	55.925901
2795.823430	181409.728846	55.930906
2795.015098	181306.491232	55.935911
2794.312671	181198.784981	55.940916
2793.883154	181087.283293	55.945921
2793.427900	180983.456279	55.950925
2792.703817	180879.761135	55.955930
2791.862464	180767.702211	55.960935
2790.852886	180656.204471	55.965940
2790.738086	180548.979185	55.970945
2789.963839	180444.262709	55.975949
2789.388892	180348.291766	55.980954
2788.851272	180234.608843	55.985959
2787.904680	180136.712914	55.990964
2787.069362	180023.700984	55.995969
2786.556424	179909.595260	56.000973
2785.519203	179806.219436	56.005978
2785.254600	179704.858430	56.010983
2784.615476	179595.912362	56.015988
2784.068819	179484.051813	56.020993
2783.470796	179382.998781	56.025997
2782.347567	179264.654011	56.031002
2782.001821	179155.331896	56.036007
2781.153224	179059.369050	56.041012
2780.645271	178950.276672	56.046017
2780.213071	178842.291905	56.051021
2779.340404	178735.839931	56.056026
2778.593295	178625.819587	56.061031
2777.741254	178532.605910	56.066036
2777.211807	178421.025286	56.071041
2776.607694	178316.096338	56.076045
2775.569311	178209.595632	56.081050
2775.302044	178099.780495	56.086055
2774.524178	178005.080798	56.091060
2774.096672	177899.412640	56.096065
2773.467072	177790.533340	56.101069
2772.857074	177683.902529	56.106074
2772.618152	177560.589191	56.111079
2771.249581	177464.623330	56.116084
2770.693082	177353.991067	56.121089
2770.195226	177246.580468	56.126093
2769.386493	177141.699611	56.131098
2768.562096	177031.123362	56.136103
2768.178799	176926.150229	56.141108
2767.252008	176822.916917	56.146113
2766.564593	176712.752272	56.151117
2765.705581	176615.194122	56.156122
2765.281444	176503.220405	56.161127
2764.321010	176405.271813	56.166132
2763.990802	176305.061430	56.171137
2763.319981	176207.359972	56.176141
2762.674152	176103.740559	56.181146
2761.846278	175987.228005	56.186151
2761.013454	175893.254111	56.191156
2760.949884	175781.746721	56.196161
2760.045471	175671.619247	56.201165
2758.947576	175575.958336	56.206170
2758.553005	175473.712491	56.211175
2757.995947	175381.553010	56.216180
2757.072149	175283.919273	56.221185
2756.578879	175179.667558	56.226189
2755.659384	175068.641097	56.231194
2755.157285	174969.008119	56.236199
2754.431391	174874.663530	56.241204
2754.072227	174773.278693	56.246209
2753.553833	174672.669714	56.251213
2752.758031	174563.392897	56.256218
2752.188094	174451.333456	56.261223
2751.501126	174350.014326	56.266228
2750.806632	174236.309128	56.271233
2750.093238	174131.204716	56.276237
2749.557877	174027.522245	56.281242
2748.636416	173916.422966	56.286247
2747.921044	173816.839342	56.291252
2747.508063	173708.101964	56.296257
2746.649463	173612.624022	56.301261
2745.984848	173514.432091	56.306266
2745.599264	173408.031296	56.311271
2744.964421	173301.059808	56.316276
2744.189995	173201.436205	56.321281
2743.430006	173096.227439	56.326285
2742.736493	172998.639097	56.331290
2742.222744	172890.441345	56.336295
2741.331769	172789.590897	56.341300
2741.195842	172679.413496	56.346305
2740.502562	172566.463215	56.351309
2739.973564	172471.991373	56.356314
2739.373325	172359.599239	56.361319
2738.712944	172249.417089	56.366324
2737.751814	172132.796955	56.371329
2737.054364	172023.689580	56.376333
2736.287308	171924.246076	56.381338
2735.450691	171803.092504	56.386343
2734.766884	171707.146368	56.391348
2734.336431	171599.282336	56.396353
2733.668123	171497.395261	56.401357
2732.845020	171397.745778	56.406362
2732.345989	171289.855311	56.411367
2731.354366	171181.941434	56.416372
2730.811128	171080.302698	56.421377
2730.006979	170975.132042	56.426381
2729.382740	170876.011947	56.431386
2729.240403	170761.173770	56.436391
2728.093440	170675.146555	56.441396
2727.486907	170565.494741	56.446401
2727.196936	170462.087990	56.451405
2726.523035	170361.222137	56.456410
2725.982850	170239.339761	56.461415
2725.017118	170141.738084	56.466420
2724.631174	170031.607750	56.471425
2724.182133	169921.284257	56.476429
2722.674429	169832.175021	56.481434
2722.157973	169706.297508	56.486439
2721.443433	169611.951016	56.491444
2720.837311	169504.858207	56.496449
2720.348770	169408.072968	56.501453
2719.403020	169300.296968	56.506458
2718.757374	169192.372000	56.511463
2718.448902	169104.511456	56.516468
2717.773142	168987.753854	56.521473
2716.949535	168896.541943	56.526477
2716.435958	168796.392358	56.531482
2716.015399	168676.772236	56.536487
2714.976993	168582.339712	56.541492
2714.461620	168474.281692	56.546497
2713.904385	168371.431569	56.551501
2713.166612	168266.028926	56.556506
2712.844208	168162.989572	56.561511
2711.832157	168060.593828	56.566516
2710.781985	167947.103213	56.571521
2710.441716	167838.586919	56.576525
2709.833464	167734.805616	56.581530
2709.221038	167619.199355	56.586535
2708.353019	167520.864104	56.591540
2707.508804	167419.651533	56.596545
2707.179590	167321.320459	56.601549
2706.312217	167214.517103	56.606554
2705.834169	167105.681418	56.611559
2705.118102	167011.913851	56.616564
2704.536097	166892.820872	56.621569
2703.666775	166799.014538	56.626573
2702.912225	166684.069461	56.631578
2702.623667	166595.524948	56.636583
2701.851758	166493.743936	56.641588
2701.130922	166385.953343	56.646593
2700.532287	166279.567848	56.651597
2699.944827	166175.660416	56.656602
2699.300957	166072.715874	56.661607
2698.327997	165967.598545	56.666612
2697.985908	165867.531320	56.671617
2697.135034	165753.354588	56.676621
2696.503394	165654.440049	56.681626
2696.038923	165550.133425	56.686631
2695.128436	165446.800539	56.691636
2694.636202	165345.130957	56.696641
2693.992061	165238.259766	56.701645
2693.295530	165128.142100	56.706650
2692.746299	165025.833954	56.711655
2692.028848	164921.759912	56.716660
2691.390289	164813.337829	56.721665
2690.991744	164706.200405	56.726669
2689.961194	164611.446104	56.731674
2689.646735	164483.952018	56.736679
2689.111517	164389.857285	56.741684
2687.884043	164276.138965	56.746689
2687.080837	164159.950680	56.751693
2686.433160	164059.123036	56.756698
2685.915567	163958.376780	56.761703
2685.152462	163859.691342	56.766708
2684.531519	163749.044547	56.771713
2683.817338	163643.219000	56.776717
2683.068353	163545.066195	56.781722
2682.517934	163439.622166	56.786727
2682.078246	163343.544242	56.791732
2681.259029	163234.774037	56.796737
2680.464729	163141.461021	56.801741
2679.924922	163031.223140	56.806746
2679.296684	162931.043988	56.811751
2678.494588	162840.174154	56.816756
2678.225116	162720.930756	56.821761
2677.599711	162615.221296	56.826765
2676.666083	162525.250382	56.831770
2676.494809	162404.314191	56.836775
2675.510677	162306.380008	56.841780
2674.981336	162192.837345	56.846785
2674.389960	162090.048295	56.851789
2674.034704	161985.632871	56.856794
2673.395995	161861.937325	56.861799
2672.603807	161756.739952	56.866804
2671.663002	161638.267638	56.871809
2671.098737	161523.842655	56.876813
2669.938425	161415.653272	56.881818
2669.458554	161312.937790	56.886823
2668.848018	161208.552369	56.891828
2668.189747	161103.272141	56.896833
2667.737592	160996.751766	56.901837
2666.945478	160893.374997	56.906842
2666.231811	160785.676174	56.911847
2665.434522	160685.148691	56.916852
2664.917419	160578.792425	56.921857
2664.671353	160469.825404	56.926861
2663.578134	160360.204699	56.931866
2663.189492	160247.599466	56.936871
2662.314842	160139.775556	56.941876
2661.702507	160028.782926	56.946881
2661.063329	159921.545334	56.951885
2660.341329	159818.389446	56.956890
2660.004707	159709.591682	56.961895
2659.051213	159609.867526	56.966900
2658.114466	159498.546574	56.971905
2657.549037	159397.248671	56.976909
2656.647657	159294.313444	56.981914
2656.368791	159171.867035	56.986919
2655.604712	159077.441162	56.991924
2655.009800	158974.521887	56.996929
2654.419011	158862.232816	57.001933
2653.565069	158761.300294	57.006938
2653.248947	158649.006530	57.011943
2652.195066	158550.648873	57.016948
2651.698927	158442.655813	57.021953
2651.226024	158326.993613	57.026957
2650.240024	158233.444237	57.031962
2649.528938	158120.108756	57.036967
2648.915546	158020.831062	57.041972
2648.514523	157907.663266	57.046977
2647.784430	157803.116246	57.051981
2646.885580	157694.579122	57.056986
2646.470766	157581.668830	57.061991
2645.378069	157493.401334	57.066996
2645.044648	157376.067599	57.072001
2644.415202	157273.616500	57.077005
2643.722349	157172.129177	57.082010
2642.980105	157071.018637	57.087015
2642.733212	156963.384796	57.092020
2641.989183	156846.842525	57.097025
2641.205705	156734.387509	57.102029
2640.471070	156633.035525	57.107034
2639.880524	156522.991365	57.112039
2639.078478	156414.913302	57.117044
2638.394239	156314.812772	57.122049
2637.850790	156206.007949	57.127053
2637.009960	156106.657425	57.132058
2636.428005	155983.622049	57.137063
2635.649596	155891.698719	57.142068
2635.223033	155783.512321	57.147073
2634.422855	155681.410848	57.152077
2633.757978	155573.911179	57.157082
2633.285399	155470.385568	57.162087
2632.709270	155364.830103	57.167092
2631.739135	155258.727239	57.172097
2631.318336	155145.584435	57.177101
2630.377666	155044.282553	57.182106
2629.948840	154934.548421	57.187111
2629.398599	154827.960903	57.192116
2628.527008	154716.492610	57.197121
2628.205589	154603.577395	57.202125
2627.387515	154505.511823	57.207130
2626.883943	154387.668776	57.212135
2625.589161	154288.014195	57.217140
2625.149827	154167.327136	57.222145
2624.660475	154066.744788	57.227149
2623.856441	153963.708511	57.232154
2623.336654	153855.441389	57.237159
2622.656817	153750.682805	57.242164
2622.207862	153642.087375	57.247169
2621.657295	153531.042472	57.252173
2620.589276	153421.351023	57.257178
2620.123935	153315.072644	57.262183
2619.211753	153203.895469	57.267188
2618.630154	153099.225057	57.272193
2618.175263	152990.264083	57.277197
2617.435736	152877.141321	57.282202
2616.797150	152769.989679	57.287207
2615.975464	152651.237169	57.292212
2615.422848	152553.351366	57.297217
2614.812732	152434.985559	57.302221
2614.051280	152338.849407	57.307226
2613.447413	152236.676513	57.312231
2612.791188	152133.762317	57.317236
2611.866710	152010.643305	57.322241
2611.614154	151909.826610	57.327245
2610.787595	151793.505640	57.332250
2610.376920	151703.302315	57.337255
2609.741178	151542.478819	57.342260
2608.770513	151409.302904	57.347265
2609.008619	151271.970444	57.352269
2607.637638	151190.461883	57.357274
2607.110371	151066.114154	57.362279
2606.354122	150975.929461	57.367284
2605.762328	150846.140214	57.372289
2605.098328	150736.304731	57.377293
2604.493273	150630.997694	57.382298
2604.020074	150511.702032	57.387303
2603.068678	150385.682865	57.392308
2602.303230	150305.720131	57.397313
2602.106879	150163.567941	57.402317
2601.190908	150061.464016	57.407322
2600.678297	149937.474150	57.412327
2599.658154	149830.583243	57.417332
2599.052336	149723.347427	57.422337
2598.644942	149606.967852	57.427341
2597.501148	149490.413071	57.432346
2597.310280	149381.879826	57.437351
2596.445350	149269.424906	57.442356
2595.953638	149153.835597	57.447361
2595.324430	149038.281200	57.452365
2594.479706	148929.637035	57.457370
2594.131742	148813.937206	57.462375
2593.434487	148695.789454	57.467380
2592.630145	148590.406276	57.472385
2591.601554	148477.026892	57.477389
2591.258797	148358.455651	57.482394
2590.656309	148226.848548	57.487399
2589.975144	148144.399601	57.492404
2589.348435	148000.088409	57.497409
2588.910130	147905.579065	57.502413
2588.121913	147789.571447	57.507418
2587.412528	147669.840827	57.512423
2586.822375	147543.343484	57.517428
2585.789948	147445.231448	57.522433
2585.159256	147303.237014	57.527437
2584.369164	147212.623456	57.532442
2584.402705	147087.477866	57.537447
2582.910776	147008.871215	57.542452
2582.681262	146843.851178	57.547457
2582.209960	146777.486717	57.552461
2580.725735	146642.213420	57.557466
2580.469087	146523.317683	57.562471
2580.071430	146402.297060	57.567476
2579.422130	146294.800097	57.572481
2578.598940	146202.479092	57.577485
2577.698912	146063.976812	57.582490
2577.441437	145976.993152	57.587495
2576.917623	145837.618941	57.592500
2575.953570	145742.983353	57.597505
2575.568780	145620.629376	57.602509
2574.604386	145497.757754	57.607514
2574.367167	145406.985544	57.612519
2573.709118	145267.762223	57.617524
2572.785132	145164.366432	57.622529
2572.443222	145020.837047	57.627533
2571.255392	144945.732818	57.632538
2570.911778	144805.419714	57.637543
2569.934506	144700.864818	57.642548
2569.060383	144593.879517	57.647553
2568.829940	144476.601255	57.652557
2568.069969	144352.392904	57.657562
2567.328403	144249.708278	57.662567
2566.859794	144124.946375	57.667572
2566.190567	144007.726718	57.672577
2565.681982	143889.135092	57.677581
2564.837615	143778.386583	57.682586
2564.613939	143662.126906	57.687591
2563.798394	143549.621080	57.692596
2562.775381	143430.032650	57.697601
2562.512024	143305.114468	57.702605
2561.714077	143188.477433	57.707610
2561.075144	143076.682350	57.712615
2560.203006	142964.911924	57.717620
2559.406795	142849.419514	57.722625
2558.853799	142718.120028	57.727629
2558.101629	142605.950703	57.732634
2557.858961	142489.723891	57.737639
2556.711743	142374.555741	57.742644
2556.085606	142239.661254	57.747649
2555.637116	142125.132995	57.752653
2554.785008	142029.347494	57.757658
2554.155318	141903.603648	57.762663
2553.727863	141804.740159	57.767668
2553.156560	141675.582722	57.772673
2552.292242	141578.313951	57.777677
2551.569450	141454.835715	57.782682
2550.930721	141329.057566	57.787687
2550.312621	141217.050006	57.792692
2549.463441	141116.883346	57.797697
2549.096209	140973.071975	57.802701
2548.075613	140885.651887	57.807706
2547.630233	140755.830421	57.812711
2546.812929	140623.654360	57.817716
2546.402284	140538.756005	57.822721
2545.811685	140383.865319	57.827725
2544.883066	140313.445231	57.832730
2544.766647	140166.675662	57.837735
2543.719576	140066.277046	57.842740
2543.258323	139926.767347	57.847745
2542.775318	139813.968568	57.852749
2541.799476	139710.713839	57.857754
2541.303993	139583.065305	57.862759
2540.612194	139472.130475	57.867764
2540.032513	139337.635476	57.872769
2539.077707	139237.555362	57.877773
2538.183208	139103.009675	57.882778
2537.814902	138984.643709	57.887783
2537.179910	138872.075862	57.892788
2536.145424	138750.830724	57.897793
2535.982270	138651.135319	57.902797
2534.977096	138509.876241	57.907802
2534.679548	138424.368846	57.912807
2534.280276	138282.290650	57.917812
2533.049449	138178.471831	57.922817
2532.890639	138047.193800	57.927821
2531.854676	137924.491245	57.932826
2531.510345	137822.349943	57.937831
2530.876521	137688.684101	57.942836
2529.689965	137560.353415	57.947841
2529.427860	137463.053438	57.952845
2528.482054	137325.081073	57.957850
2527.916571	137200.426726	57.962855
2527.193537	137088.171837	57.967860
2526.762370	136972.580725	57.972865
2526.172863	136861.207542	57.977869
2525.432776	136739.796984	57.982874
2524.679885	136600.908167	57.987879
2524.266352	136511.753242	57.992884
2523.308551	136368.261041	57.997889
2522.661251	136252.579993	58.002893
2522.157966	136135.631601	58.007898
2521.681027	135998.772644	58.012903
2520.944766	135886.613399	58.017908
2519.720531	135769.882373	58.022913
2519.314362	135646.467078	58.027917
2518.691483	135538.203931	58.032922
2518.043812	135419.998241	58.037927
2517.442301	135293.121936	58.042932
2516.650109	135173.225189	58.047937
2516.211080	135052.104253	58.052941
2515.360141	134946.839354	58.057946
2515.352313	134795.645884	58.062951
2514.393708	134710.368461	58.067956
2513.514564	134557.840762	58.072961
2513.092061	134452.331920	58.077965
2512.590484	134303.480444	58.082970
2511.686613	134204.692504	58.087975
2511.010479	134064.660416	58.092980
2510.314508	133947.814932	58.097985
2509.859948	133817.758815	58.102989
2508.662869	133716.935765	58.107994
2508.312546	133581.478217	58.112999
2507.596561	133456.851135	58.118004
2506.654544	133333.403660	58.123009
2506.350187	133225.200358	58.128013
2505.707640	133101.211022	58.133018
2504.909685	132972.038847	58.138023
2504.396564	132862.612467	58.143028
2503.790802	132731.035573	58.148033
2503.287437	132598.083913	58.153037
2502.448270	132486.373438	58.158042
2501.917075	132356.844223	58.163047
2501.264441	132221.923742	58.168052
2500.372557	132117.603014	58.173057
2500.031222	131972.320294	58.178061
2498.855040	131844.356389	58.183066
2498.253617	131734.376774	58.188071
2497.834876	131610.129851	58.193076
2496.995476	131492.580491	58.198081
2496.629749	131364.896761	58.203085
2495.429699	131235.643827	58.208090
2495.149937	131118.350272	58.213095
2494.390548	130997.106828	58.218100
2493.799979	130876.967585	58.223105
2493.260547	130742.480799	58.228109
2492.233224	130641.578303	58.233114
2492.024540	130497.857145	58.238119
2491.424799	130363.508751	58.243124
2490.484766	130265.375361	58.248129
2490.159440	130117.762661	58.253133
2489.272675	130003.935798	58.258138
2488.625630	129875.655688	58.263143
2487.655868	129748.849835	58.268148
2486.918841	129621.296418	58.273153
2486.356500	129515.320124	58.278157
2485.525687	129376.758313	58.283162
2485.148237	129250.648302	58.288167
2484.332513	129146.110667	58.293172
2483.789227	128998.157435	58.298177
2483.280273	128891.311418	58.303181
2482.671885	128772.009620	58.308186
2482.137449	128631.283568	58.313191
2481.629625	128516.488311	58.318196
2480.699863	128389.783945	58.323201
2480.338313	128239.608801	58.328205
2479.184417	128159.411524	58.333210
2478.712289	127998.675890	58.338215
2478.189523	127888.419593	58.343220
2477.651471	127766.329667	58.348225
2476.714867	127618.166784	58.353229
2475.909773	127499.485883	58.358234
2475.630364	127375.489803	58.363239
2474.451069	127240.727748	58.368244
2473.767373	127139.986765	58.373249
2473.447526	126988.529176	58.378253
2472.671315	126868.614561	58.383258
2472.092457	126764.023044	58.388263
2471.298551	126632.187320	58.393268
2470.988040	126493.468673	58.398273
2470.350961	126379.617222	58.403277
2469.836289	126246.532656	58.408282
2469.165035	126098.234370	58.413287
2468.234857	125971.058708	58.418292
2467.468299	125850.943863	58.423297
2466.895556	125712.131083	58.428301
2466.342188	125589.583466	58.433306
2465.553123	125472.343863	58.438311
2464.832182	125341.252091	58.443316
2464.296796	125222.093916	58.448321
2463.510278	125089.769268	58.453325
2463.066118	124961.124444	58.458330
2462.675424	124807.087011	58.463335
2461.645704	124706.460719	58.468340
2461.165205	124569.150338	58.473345
2460.696498	124428.346692	58.478349
2459.885072	124315.052222	58.483354
2459.507569	124169.791005	58.488359
2458.612275	124027.368197	58.493364
2457.583947	123907.189237	58.498369
2456.973285	123749.675317	58.503373
2455.779538	123677.078479	58.508378
2455.402561	123504.799073	58.513383
2454.761345	123403.595475	58.518388
2454.109416	123263.017479	58.523393
2453.873658	123136.710207	58.528397
2452.965149	123019.373290	58.533402
2452.656210	122893.980319	58.538407
2451.661920	122750.424527	58.543412
2451.212673	122630.184931	58.548417
2450.671405	122511.915903	58.553421
2449.480352	122352.229386	58.558426
2449.394926	122232.467218	58.563431
2448.451961	122083.040667	58.568436
2447.768977	121992.070502	58.573441
2447.134581	121826.864441	58.578445
2446.507658	121714.694563	58.583450
2445.981671	121558.310282	58.588455
2445.264594	121457.164240	58.593460
2444.687612	121301.830730	58.598465
2443.824192	121195.007924	58.603469
2443.044801	121038.349480	58.608474
2442.539355	120938.962152	58.613479
2442.144821	120776.492580	58.618484
2441.188560	120669.166067	58.623489
2440.765234	120517.215570	58.628493
2440.043103	120385.665968	58.633498
2439.216682	120264.068604	58.638503
2438.847909	120138.806153	58.643508
2438.047102	119991.533726	58.648513
2437.453155	119868.834854	58.653517
2436.356960	119709.942903	58.658522
2435.791555	119605.237722	58.663527
2435.248421	119476.787604	58.668532
2434.373212	119337.326119	58.673537
2433.553217	119211.676255	58.678541
2432.674693	119097.246821	58.683546
2432.207000	118965.092750	58.688551
2431.845942	118825.679470	58.693556
2431.227701	118729.219457	58.698561
2431.063453	118578.362793	58.703565
2429.683222	118446.978125	58.708570
2429.414709	118332.283982	58.713575
2428.682382	118176.308184	58.718580
2427.863874	118060.959751	58.723585
2427.505579	117909.261776	58.728589
2426.525245	117801.106713	58.733594
2425.773112	117632.689577	58.738599
2425.192730	117557.625809	58.743604
2424.863163	117390.527051	58.748609
2424.205013	117295.246693	58.753613
2422.847416	117151.550836	58.758618
2422.705958	117013.039298	58.763623
2421.832168	116895.933927	58.768628
2421.494834	116754.363637	58.773633
2420.793153	116612.001346	58.778637
2420.140856	116506.637028	58.783642
2419.543751	116350.136777	58.788647
2418.965835	116212.041533	58.793652
2417.888144	116107.831690	58.798657
2417.562957	115944.753159	58.803661
2416.466951	115827.084951	58.808666
2416.326391	115690.979688	58.813671
2415.802526	115557.214535	58.818676
2415.023708	115429.964528	58.823681
2414.346870	115282.502698	58.828685
2413.446659	115156.802948	58.833690
2412.957574	115025.954715	58.838695
2412.399862	114861.047667	58.843700
2411.539841	114763.796831	58.848705
2411.323762	114590.967219	58.853709
2410.035325	114493.239519	58.858714
2409.576129	114317.752917	58.863719
2409.022253	114225.761551	58.868724
2408.386354	114066.920579	58.873729
2408.052400	113928.418335	58.878733
2406.880855	113819.777446	58.883738
2406.605106	113650.555978	58.888743
2405.757673	113524.303868	58.893748
2405.008663	113388.218657	58.898753
2404.597763	113241.399376	58.903757
2403.640446	113129.884281	58.908762
2402.990011	112983.745488	58.913767
2402.386107	112834.566586	58.918772
2401.445621	112720.061492	58.923777
2401.314343	112577.428489	58.928781
2400.428918	112440.094465	58.933786
2399.815755	112319.954558	58.938791
2399.200995	112169.137680	58.943796
2398.678423	112042.283113	58.948801
2397.909664	111899.342568	58.953805
2397.532674	111753.649969	58.958810
2396.450039	111604.135517	58.963815
2395.933147	111470.568799	58.968820
2395.000510	111347.996600	58.973825
2394.771306	111198.241416	58.978829
2393.814300	111067.640436	58.983834
2393.270189	110942.857370	58.988839
2392.675911	110784.170391	58.993844
2391.939261	110646.975051	58.998849
2391.377309	110520.508957	59.003853
2390.666914	110378.519854	59.008858
2389.742174	110236.552865	59.013863
2389.308187	110116.687190	59.018868
2388.483712	109958.962176	59.023873
2387.700967	109831.697014	59.028877
2387.171994	109697.761110	59.033882
2386.819407	109552.001542	59.038887
2386.092314	109417.870144	59.043892
2385.350454	109284.262158	59.048897
2384.805683	109138.059621	59.053901
2384.193443	109009.781822	59.058906
2383.629375	108854.732164	59.063911
2382.898588	108721.233386	59.068916
2381.851749	108568.895421	59.073921
2381.246384	108455.829201	59.078925
2380.098621	108302.182749	59.083930
2380.070118	108140.022206	59.088935
2378.970800	108052.873893	59.093940
2378.238111	107906.689537	59.098945
2377.976062	107774.917335	59.103949
2377.264404	107625.603205	59.108954
2376.503076	107514.710750	59.113959
2375.865978	107364.840740	59.118964
2374.954543	107239.735162	59.123969
2375.071716	107077.292169	59.128973
2373.742057	106966.422560	59.133978
2373.261296	106822.609556	59.138983
2372.824240	106681.893104	59.143988
2371.734239	106545.760426	59.148993
2371.449987	106403.320978	59.153997
2370.831860	106290.317706	59.159002
2370.183059	106126.384694	59.164007
2369.345741	106000.195240	59.169012
2368.362888	105856.619919	59.174017
2368.084919	105744.015765	59.179021
2367.331099	105591.865924	59.184026
2366.452744	105474.809204	59.189031
2365.816197	105324.818642	59.194036
2365.339078	105196.146405	59.199041
2364.914600	105054.530295	59.204045
2364.573840	104940.296700	59.209050
2363.873264	104775.569116	59.214055
2362.574923	104626.176412	59.219060
2361.958893	104505.073297	59.224065
2361.748373	104358.358367	59.229069
2360.807042	104208.163080	59.234074
2359.911905	104102.871541	59.239079
2359.275672	103933.730441	59.244084
2358.898269	103823.847406	59.249089
2358.428135	103666.532600	59.254093
2357.668136	103523.843274	59.259098
2356.834763	103401.803310	59.264103
2356.584146	103261.540668	59.269108
2355.365775	103130.332769	59.274113
2355.411533	102976.195188	59.279117
2354.091669	102825.840366	59.284122
2353.281438	102694.373535	59.289127
2353.169775	102549.620765	59.294132
2352.262747	102418.107397	59.299137
2352.050996	102275.789135	59.304141
2350.812036	102130.272505	59.309146
2350.443069	101998.910895	59.314151
2349.944018	101854.877240	59.319156
2348.934874	101710.804832	59.324161
2348.412343	101571.140979	59.329165
2347.356532	101435.990228	59.334170
2347.129511	101288.732547	59.339175
2346.305067	101147.660134	59.344180
2345.526669	101026.105964	59.349185
2345.013879	100872.330917	59.354189
2344.186057	100737.649202	59.359194
2343.554492	100595.287266	59.364199
2342.958933	100454.563372	59.369204
2342.231044	100322.062962	59.374209
2341.968319	100180.228663	59.379213
2340.869450	100051.099718	59.384218
2340.552546	99905.209813	59.389223
2339.913652	99756.504871	59.394228
2339.024292	99620.228325	59.399233
2338.548766	99475.590477	59.404237
2337.792072	99356.813497	59.409242
2337.100609	99209.750539	59.414247
2336.385015	99076.158047	59.419252
2335.463258	98922.213490	59.424257
2334.960727	98804.781782	59.429261
2334.452393	98658.067544	59.434266
2333.619091	98519.942937	59.439271
2333.024825	98381.711493	59.444276
2332.514413	98226.298341	59.449281
2332.226665	98099.322400	59.454285
2331.058912	97969.829217	59.459290
2330.962098	97799.512030	59.464295
2329.808732	97693.808550	59.469300
2329.211418	97527.143530	59.474305
2328.459113	97393.693553	59.479309
2327.964467	97245.013784	59.484314
2326.904440	97094.058995	59.489319
2326.716468	96965.741694	59.494324
2325.929419	96822.539972	59.499329
2325.269222	96683.771196	59.504333
2324.259346	96551.121738	59.509338
2323.648279	96418.447870	59.514343
2323.040219	96273.109350	59.519348
2322.229913	96137.094792	59.524353
2321.765503	96002.567290	59.529357
2321.183735	95856.732615	59.534362
2320.737751	95726.750960	59.539367
2320.157028	95590.576461	59.544372
2319.689262	95445.544465	59.549377
2318.780806	95307.229406	59.554381
2318.159661	95151.797850	59.559386
2317.296698	95013.230066	59.564391
2316.792849	94867.338726	59.569396
2316.095634	94716.082341	59.574401
2315.328769	94577.362503	59.579405
2314.399726	94432.219969	59.584410
2313.952679	94279.550768	59.589415
2313.428840	94170.212815	59.594420
2312.618623	94011.699201	59.599425
2312.395610	93880.348540	59.604429
2311.306734	93724.639630	59.609434
2310.799463	93598.954071	59.614439
2310.121846	93429.294719	59.619444
2309.064901	93325.720817	59.624449
2309.071581	93157.800298	59.629453
2308.535517	93020.835412	59.634458
2307.927175	92871.682699	59.639463
2307.115728	92719.462461	59.644468
2306.098751	92582.208776	59.649473
2305.530299	92419.445132	59.654477
2305.057875	92304.661390	59.659482
2304.280549	92140.715479	59.664487
2303.618634	92002.248726	59.669492
2302.924749	91867.915733	59.674497
2302.217357	91717.233048	59.679501
2301.435502	91553.938975	59.684506
2301.015824	91436.025458	59.689511
2300.320092	91284.544974	59.694516
2299.785281	91141.377807	59.699521
2299.225383	90995.660338	59.704525
2298.152899	90847.755249	59.709530
2297.860758	90683.280419	59.714535
2296.956300	90554.771301	59.719540
2295.947249	90428.733230	59.724545
2295.683063	90266.843951	59.729549
2295.133569	90125.365935	59.734554
2294.119039	89983.315886	59.739559
2293.416447	89854.151205	59.744564
2292.753614	89707.811957	59.749569
2292.444586	89550.227367	59.754573
2291.083244	89421.353588	59.759578
2290.651859	89272.565016	59.764583
2290.259497	89129.553301	59.769588
2289.368083	89003.213200	59.774593
2288.746041	88863.124325	59.779597
2288.316948	88719.613951	59.784602
2287.630219	88570.838991	59.789607
2286.992178	88438.781563	59.794612
2286.159179	88283.875889	59.799617
2285.975010	88138.073602	59.804621
2284.727463	88013.488455	59.809626
2284.424345	87874.445826	59.814631
2283.762648	87715.859134	59.819636
2282.737198	87576.153226	59.824641
2282.031025	87440.042773	59.829645
2281.390515	87318.015274	59.834650
2280.708496	87166.535999	59.839655
2280.200037	87017.908320	59.844660
2279.613477	86875.303693	59.849665
2279.195053	86746.885926	59.854669
2278.093254	86586.272751	59.859674
2277.688240	86464.998822	59.864679
2277.374923	86315.235719	59.869684
2276.154697	86171.855143	59.874689
2275.454232	86024.038187	59.879693
2275.101543	85889.016224	59.884698
2274.384415	85733.387957	59.889703
2273.677468	85601.650521	59.894708
2273.108577	85469.765228	59.899713
2272.643719	85306.918142	59.904718
2271.692317	85164.357461	59.909722
2270.906321	85024.509838	59.914727
2270.437847	84885.874177	59.919732
2269.977778	84745.114644	59.924737
2269.273848	84599.488643	59.929742
2268.599401	84453.497670	59.934746
2267.990119	84310.476473	59.939751
2267.264497	84152.813811	59.944756
2266.427969	84018.450952	59.949761
2266.227868	83860.669096	59.954766
2265.340992	83725.238566	59.959770
2264.862603	83574.836447	59.964775
2264.180307	83424.556477	59.969780
2263.585934	83271.462150	59.974785
2263.017501	83132.099616	59.979790
2261.796438	82989.590061	59.984794
2261.201764	82836.346840	59.989799
2260.892855	82691.216458	59.994804
2259.702438	82550.346580	59.999809
2259.443883	82390.068855	60.004814
2258.379787	82257.464602	60.009818
2257.773492	82131.215171	60.014823
2257.351064	81977.177705	60.019828
2256.736196	81821.505065	60.024833
2256.144508	81673.137300	60.029838
2255.642064	81536.164255	60.034842
2254.886100	81380.929234	60.039847
2254.521948	81236.559226	60.044852
2253.300622	81095.830833	60.049857
2252.556963	80932.580218	60.054862
2252.083010	80791.767038	60.059866
2251.271195	80650.697868	60.064871
2250.628842	80501.161412	60.069876
2249.702092	80368.312945	60.074881
2249.242888	80218.895238	60.079886
2248.718719	80073.715848	60.084890
2247.896940	79926.569455	60.089895
2247.299284	79785.446873	60.094900
2246.637945	79642.256787	60.099905
2246.478711	79493.740978	60.104910
2245.527649	79347.252930	60.109914
2244.694517	79218.592120	60.114919
2244.121293	79058.567471	60.119924
2243.452718	78908.279955	60.124929
2242.901184	78759.692254	60.129934
2241.967193	78631.672127	60.134938
2241.642736	78472.765883	60.139943
2240.957075	78321.566548	60.144948
2240.060754	78200.120632	60.149953
2239.758332	78030.917260	60.154958
2238.760173	77877.901472	60.159962
2238.040194	77748.161071	60.164967
2237.577429	77580.513960	60.169972
2236.484481	77440.778707	60.174977
2236.207750	77315.628022	60.179982
2235.678072	77155.814112	60.184986
2235.078855	77004.059565	60.189991
2234.443933	76850.271546	60.194996
2233.422407	76713.393942	60.200001
2233.085893	76574.672504	60.205006
2232.807769	76424.201951	60.210010
2231.950050	76249.354613	60.215015
2231.242173	76121.928992	60.220020
2230.290707	75967.513587	60.225025
2229.944440	75804.912410	60.230030
2229.141462	75678.765513	60.235034
2228.381843	75510.631361	60.240039
2227.612845	75365.448248	60.245044
2226.842999	75223.427842	60.250049
2226.310324	75059.493721	60.255054
2225.831902	74921.889533	60.260058
2225.167312	74781.325417	60.265063
2224.267476	74615.495455	60.270068
2223.698855	74487.335828	60.275073
2223.490920	74318.503249	60.280078
2222.088056	74187.633249	60.285082
2221.911294	74018.975638	60.290087
2221.332920	73874.425604	60.295092
2220.031620	73728.166730	60.300097
2219.391191	73579.738823	60.305102
2218.906119	73456.621700	60.310106
2218.389522	73281.486317	60.315111
2217.578006	73169.021397	60.320116
2216.824827	72995.617517	60.325121
2216.237277	72861.269327	60.330126
2215.633582	72726.443150	60.335130
2214.871312	72546.253574	60.340135
2214.242972	72434.435248	60.345140
2213.671300	72265.449667	60.350145
2213.285618	72135.844457	60.355150
2212.605056	71970.951900	60.360154
2211.839343	71835.923085	60.365159
2211.346430	71694.181576	60.370164
2210.343744	71524.079778	60.375169
2209.892024	71398.512309	60.380174
2209.329349	71233.391824	60.385178
2208.264302	71086.088756	60.390183
2207.727731	70961.253315	60.395188
2207.111244	70811.581769	60.400193
2206.368824	70643.188219	60.405198
2205.803584	70510.670377	60.410202
2205.326935	70351.187434	60.415207
2204.402076	70218.525912	60.420212
2203.873815	70057.432001	60.425217
2203.153885	69926.709844	60.430222
2202.729930	69749.766818	60.435226
2201.936783	69627.723159	60.440231
2201.700696	69452.988894	60.445236
2200.861681	69315.645457	60.450241
2200.344793	69164.786237	60.455246
2199.738187	68998.336072	60.460250
2198.503463	68863.813760	60.465255
2198.038804	68702.429560	60.470260
2197.370971	68548.951580	60.475265
2196.783533	68385.911074	60.480270
2195.919558	68259.004049	60.485274
2195.201714	68112.105287	60.490279
2194.999222	67947.607696	60.495284
2194.041194	67804.220064	60.500289
2193.317094	67651.853760	60.505294
2192.548432	67501.541362	60.510298
2191.892890	67361.915303	60.515303
2191.641635	67203.970788	60.520308
2190.594529	67068.392516	60.525313
2189.905529	66918.372832	60.530318
2189.650742	66763.295019	60.535322
2188.860858	66597.163658	60.540327
2188.186494	66441.819337	60.545332
2187.448397	66313.838000	60.550337
2186.829218	66138.491361	60.555342
2186.215338	65995.027730	60.560346
2185.319076	65865.412114	60.565351
2185.019382	65695.468135	60.570356
2183.837690	65546.920972	60.575361
2183.730414	65390.956904	60.580366
2182.963645	65262.816133	60.585370
2181.930148	65084.916840	60.590375
2181.391998	64953.942922	60.595380
2180.954705	64798.599609	60.600385
2180.378380	64635.069770	60.605390
2179.478009	64503.643479	60.610394
2178.516418	64357.749181	60.615399
2178.172297	64167.242939	60.620404
2177.506655	64058.014692	60.625409
2176.967461	63890.002206	60.630414
2176.345801	63735.342662	60.635418
2175.351073	63602.911766	60.640423
2175.222765	63448.287101	60.645428
2173.921301	63290.588890	60.650433
2173.306873	63154.925358	60.655438
2172.922828	62990.650975	60.660442
2171.976339	62833.802526	60.665447
2171.716630	62698.728653	60.670452
2170.898458	62541.365235	60.675457
2170.078948	62409.104830	60.680462
2169.818299	62246.162786	60.685466
2168.732478	62105.956380	60.690471
2168.451347	61943.504552	60.695476
2167.347570	61798.105194	60.700481
2166.974759	61649.887524	60.705486
2166.421967	61494.456606	60.710490
2165.274581	61357.184252	60.715495
2164.901943	61185.649185	60.720500
2164.225534	61047.345206	60.725505
2163.679001	60893.675144	60.730510
2162.657671	60752.468286	60.735514
2161.888821	60628.322385	60.740519
2161.778687	60471.756602	60.745524
2161.041146	60306.415788	60.750529
2160.287093	60164.854416	60.755534
2160.030716	60005.457368	60.760538
2158.931618	59861.819563	60.765543
2158.912434	59698.367501	60.770548
2157.537171	59569.858553	60.775553
2157.088570	59385.674970	60.780558
2156.639259	59246.205612	60.785562
2155.878611	59107.824886	60.790567
2155.605728	58947.898235	60.795572
2154.493329	58793.933231	60.800577
2153.741129	58635.917942	60.805582
2153.145161	58474.327946	60.810586
2152.561806	58327.290459	60.815591
2151.928219	58187.801306	60.820596
2151.286266	58024.839385	60.825601
2150.227061	57853.921781	60.830606
2149.401717	57731.351850	60.835610
2149.008350	57557.036598	60.840615
2148.521364	57411.747649	60.845620
2147.665877	57282.510624	60.850625
2147.350932	57107.813708	60.855630
2146.285753	56964.079027	60.860634
2145.558188	56834.271000	60.865639
2145.365672	56664.818823	60.870644
2144.381649	56509.096016	60.875649
2143.971268	56372.433475	60.880654
2143.340514	56198.808010	60.885658
2142.576834	56055.187675	60.890663
2142.042015	55910.740984	60.895668
2140.999206	55758.119440	60.900673
2140.867069	55588.822676	60.905678
2139.688063	55461.827048	60.910682
2139.279967	55296.174927	60.915687
2138.655265	55132.745372	60.920692
2137.584056	54982.065185	60.925697
2137.136084	54854.407173	60.930702
2136.546150	54692.542470	60.935706
2135.926161	54542.563292	60.940711
2135.560980	54373.615381	60.945716
2134.645453	54243.877695	60.950721
2134.201239	54057.569586	60.955726
2133.538577	53938.612910	60.960730
2132.661512	53750.000209	60.965735
2132.144327	53625.655840	60.970740
2131.364128	53452.336518	60.975745
2130.557700	53315.648948	60.980750
2129.912860	53132.328066	60.985754
2129.053516	53017.249979	60.990759
2129.073088	52829.400065	60.995764
2127.817625	52718.091946	61.000769
2127.480322	52526.270705	61.005774
2126.699868	52391.405357	61.010778
2126.049462	52237.741784	61.015783
2125.806617	52064.847264	61.020788
2125.019908	51931.998657	61.025793
2124.348675	51743.848832	61.030798
2123.620790	51622.845357	61.035802
2123.200712	51431.203939	61.040807
2122.421091	51291.382544	61.045812
2121.455093	51149.161972	61.050817
2120.789907	50968.710630	61.055822
2120.067417	50837.698111	61.060826
2119.412851	50649.269210	61.065831
2118.778498	50533.045024	61.070836
2118.139054	50362.846231	61.075841
2117.471473	50199.765481	61.080846
2116.835566	50078.435152	61.085850
2116.182089	49905.212159	61.090855
2115.278625	49739.363739	61.095860
2114.863958	49612.487321	61.100865
2114.149480	49432.628758	61.105870
2113.591739	49299.453342	61.110874
2112.861346	49154.936702	61.115879
2112.688578	48973.756737	61.120884
2111.524294	48833.613869	61.125889
2111.258111	48683.058005	61.130894
2110.318850	48514.180329	61.135898
2109.637244	48358.713967	61.140903
2109.025515	48223.252270	61.145908
2108.292423	48038.007824	61.150913
2107.515302	47903.280236	61.155918
2107.073780	47728.659333	61.160922
2106.228933	47578.169884	61.165927
2105.911234	47425.934240	61.170932
2104.925949	47286.357264	61.175937
2104.580252	47116.108201	61.180942
2103.625307	46961.735016	61.185946
2102.935060	46803.225001	61.190951
2102.283408	46646.060912	61.195956
2101.373721	46504.766935	61.200961
2101.221857	46343.670525	61.205966
2100.413701	46183.141520	61.210970
2099.289737	46052.503264	61.215975
2099.175474	45879.303739	61.220980
2098.390027	45721.150709	61.225985
2097.750027	45572.543666	61.230990
2097.113589	45426.644702	61.235994
2096.372564	45267.252063	61.240999
2095.844863	45097.424679	61.246004
2095.127815	44939.723308	61.251009
2094.183855	44790.633484	61.256014
2093.782373	44638.925547	61.261018
2093.044948	44490.934596	61.266023
2092.324871	44333.489044	61.271028
2091.459899	44181.264066	61.276033
2090.948593	44025.261953	61.281038
2090.423631	43874.377245	61.286042
2089.591508	43706.670553	61.291047
2089.395263	43563.636357	61.296052
2088.092703	43419.042692	61.301057
2087.726173	43257.401651	61.306062
2087.265697	43107.895367	61.311066
2086.454376	42949.825399	61.316071
2085.763786	42792.626341	61.321076
2085.067454	42641.640424	61.326081
2084.612515	42488.125636	61.331086
2083.656049	42339.428871	61.336090
2082.942668	42175.048062	61.341095
2082.480535	42011.264558	61.346100
2081.292735	41880.427509	61.351105
2081.115794	41715.026803	61.356110
2080.293867	41570.603212	61.361114
2079.771978	41419.505467	61.366119
2079.268299	41268.855177	61.371124
2078.541553	41108.572082	61.376129
2077.693796	40958.459746	61.381134
2077.063581	40805.803590	61.386138
2076.624406	40647.770032	61.391143
2075.908259	40505.093519	61.396148
2074.989809	40350.613719	61.401153
2074.603235	40177.059143	61.406158
2073.711029	40048.864124	61.411162
2073.156545	39880.548346	61.416167
2072.637389	39725.364254	61.421172
2071.730441	39584.646498	61.426177
2071.432432	39424.556202	61.431182
2070.664654	39251.770276	61.436186
2069.916733	39128.018869	61.441191
2069.723206	38953.527652	61.446196
2068.472716	38798.275207	61.451201
2067.703250	38662.962272	61.456206
2067.426195	38481.110021	61.461210
2066.384085	38330.966315	61.466215
2065.615768	38188.326992	61.471220
2065.040466	38039.784227	61.476225
2064.659727	37881.741791	61.481230
2063.828076	37731.682240	61.486234
2063.022204	37584.928323	61.491239
2062.585980	37416.910641	61.496244
2061.997100	37272.146697	61.501249
2061.353133	37113.685343	61.506254
2060.349744	36962.885367	61.511258
2059.836914	36816.276573	61.516263
2059.150573	36672.206596	61.521268
2058.477685	36522.709540	61.526273
2057.969718	36359.404995	61.531278
2057.374281	36219.008806	61.536282
2056.944747	36058.332705	61.541287
2056.326491	35899.578411	61.546292
2055.256658	35751.731749	61.551297
2054.921589	35594.933181	61.556302
2054.152090	35437.389487	61.561306
2053.593980	35277.218589	61.566311
2052.884652	35124.439754	61.571316
2052.074291	34959.695402	61.576321
2051.537302	34798.059093	61.581326
2050.737423	34657.310183	61.586330
2050.224867	34501.638946	61.591335
2049.502643	34331.063035	61.596340
2048.804041	34178.890128	61.601345
2048.122859	34019.635847	61.606350
2047.653780	33874.093672	61.611354
2046.923875	33726.392764	61.616359
2046.273107	33570.900723	61.621364
2045.341048	33419.350216	61.626369
2045.123429	33254.675651	61.631374
2044.507510	33084.389606	61.636378
2043.734200	32938.960804	61.641383
2043.149931	32771.800275	61.646388
2042.205020	32625.440678	61.651393
2041.424822	32451.859261	61.656398
2041.109334	32298.475046	61.661402
2040.121746	32140.200811	61.666407
2039.811879	31977.061095	61.671412
2038.957487	31847.416900	61.676417
2038.360997	31669.545000	61.681422
2037.737002	31509.686394	61.686426
2037.035197	31371.822504	61.691431
2036.310744	31202.890906	61.696436
2035.407641	31048.075743	61.701441
2034.640067	30881.597088	61.706446
2034.150726	30740.694772	61.711450
2033.343862	30594.527257	61.716455
2032.874100	30428.950793	61.721460
2031.776968	30271.737375	61.726465
2031.674332	30128.438977	61.731470
2031.150565	29971.838962	61.736474
2029.888898	29820.462385	61.741479
2029.189035	29669.146569	61.746484
2028.759499	29512.393810	61.751489
2028.356488	29364.650154	61.756494
2027.440643	29213.047384	61.761498
2026.578877	29060.470557	61.766503
2026.185757	28913.944347	61.771508
2025.393977	28763.692659	61.776513
2025.075891	28604.986146	61.781518
2024.619589	28448.961957	61.786522
2023.374953	28304.893975	61.791527
2022.915031	28148.762659	61.796532
2022.203313	28004.890810	61.801537
2021.319453	27844.753875	61.806542
2020.868663	27692.859267	61.811546
2020.548267	27541.411410	61.816551
2019.887840	27386.476417	61.821556
2018.379208	27245.839568	61.826561
2018.047971	27083.433787	61.831566
2017.069633	26927.642170	61.836570
2016.599318	26775.470991	61.841575
2016.255654	26630.657294	61.846580
2015.515268	26486.703205	61.851585
2014.701082	26342.497530	61.856590
2014.091046	26195.322688	61.861594
2013.229935	26046.269842	61.866599
2012.955349	25892.073820	61.871604
2012.003535	25750.331789	61.876609
2011.582656	25603.613320	61.881614
2011.128491	25454.407399	61.886618
2010.179311	25289.395473	61.891623
2009.403147	25140.563428	61.896628
2008.752382	25013.430774	61.901633
2008.298234	24839.313426	61.906638
2007.416984	24699.671765	61.911642
2006.512882	24560.422705	61.916647
2006.426938	24394.383515	61.921652
2005.409791	24252.098900	61.926657
2004.751457	24111.566225	61.931662
2004.394369	23964.119825	61.936666
2003.266172	23815.171215	61.941671
2002.657778	23653.779125	61.946676
2001.682181	23518.941107	61.951681
2001.543608	23379.736428	61.956686
2000.766492	23233.682981	61.961690
2000.007647	23096.063783	61.966695
1999.501677	22939.513494	61.971700
1998.473058	22799.761065	61.976705
1998.092488	22653.064906	61.981710
1997.347323	22505.952619	61.986714
1996.632259	22362.423336	61.991719
1995.854950	22230.411349	61.996724
1995.102904	22078.182755	62.001729
1994.809648	21931.815786	62.006734
1994.396414	21780.469579	62.011738
1993.177308	21669.183148	62.016743
1993.034185	21490.205117	62.021748
1991.980391	21355.069477	62.026753
1991.137993	21233.948410	62.031758
1990.885977	21078.030778	62.036762
1989.959783	20928.876721	62.041767
1989.132733	20810.048513	62.046772
1988.531901	20653.507897	62.051777
1987.722124	20525.952863	62.056782
1987.436270	20370.272232	62.061786
1986.094284	20246.074497	62.066791
1986.151424	20089.882713	62.071796
1985.496990	19966.026502	62.076801
1984.542976	19827.346113	62.081806
1984.269699	19673.166078	62.086810
1983.552790	19529.448571	62.091815
1982.842903	19390.038180	62.096820
1981.918102	19245.721549	62.101825
1981.337018	19110.364428	62.106830
1980.330424	18974.838001	62.111834
1979.496721	18838.806518	62.116839
1979.051324	18707.654827	62.121844
1978.216527	18568.936686	62.126849
1977.333154	18446.562443	62.131854
1976.980629	18310.406306	62.136858
1975.969619	18204.035400	62.141863
1975.504782	18055.053384	62.146868
1974.511115	17931.140463	62.151873
1973.539511	17792.482929	62.156878
1973.304805	17671.410610	62.161882
1972.010354	17569.419554	62.166887
1971.669325	17433.923654	62.171892
1970.448200	17334.762042	62.176897
1969.299789	17232.504535	62.181902
1968.716407	17105.707991	62.186906
1967.712154	17030.283715	62.191911
1966.914663	16936.618333	62.196916
1965.321040	16832.418764	62.201921
1964.781068	16768.093896	62.206926
1964.067317	16669.568584	62.211930
1962.572321	16619.510235	62.216935
1961.966260	16557.001127	62.221940
1960.761196	16479.081260	62.226945
1959.974552	16451.824641	62.231950
1959.180109	16382.867658	62.236954
1958.529986	16328.641990	62.241959
1958.093354	16266.490374	62.246964
1957.131295	16227.463492	62.251969
1956.711739	16184.257288	62.256974
1956.071463	16145.004116	62.261978
1955.236850	16080.312730	62.266983
1954.744473	16042.895722	62.271988
1954.034969	15987.811275	62.276993
1953.410780	15952.208479	62.281998
1953.005050	15883.095148	62.287002
1952.470031	15826.905912	62.292007
1951.730327	15796.438625	62.297012
1951.105088	15741.906511	62.302017
1950.617863	15671.191616	62.307022
1950.117733	15633.102402	62.312026
1949.199724	15563.515486	62.317031
1948.965987	15520.721173	62.322036
1948.282117	15476.630935	62.327041
1947.534682	15400.660956	62.332046
1946.675938	15360.791849	62.337050
1946.552765	15279.303745	62.342055
1945.925076	15257.771954	62.347060
1944.986609	15176.288520	62.352065
1944.346388	15130.816886	62.357070
1943.793261	15070.381923	62.362074
1942.749883	15017.196740	62.367079
1942.421354	14963.092950	62.372084
1941.776812	14909.251522	62.377089
1940.955587	14850.554667	62.382094
1940.545162	14788.616578	62.387098
1939.857145	14744.034853	62.392103
1939.580285	14695.041442	62.397108
1938.919760	14615.035462	62.402113
1937.946721	14586.635030	62.407118
1937.649242	14497.329783	62.412122
1936.723864	14434.689504	62.417127
1936.215643	14390.895521	62.422132
1935.686426	14322.911832	62.427137
1934.811087	14256.037070	62.432142
1933.775545	14207.888955	62.437146
1932.989947	14163.114193	62.442151
1932.731673	14092.831122	62.447156
1931.927980	14044.992088	62.452161
1931.404743	13988.510789	62.457166
1930.938768	13918.074257	62.462170
1930.340911	13875.101048	62.467175
1929.818647	13820.267336	62.472180
1928.940666	13758.078628	62.477185
1928.400892	13697.427480	62.482190
1927.707065	13630.012306	62.487194
1926.744408	13581.652871	62.492199
1926.316219	13513.725404	62.497204
1925.720296	13487.765551	62.502209
1924.989035	13401.180834	62.507214
1924.160342	13347.739820	62.512218
1923.289727	13294.982346	62.517223
1923.055863	13251.211807	62.522228
1922.056493	13180.131422	62.527233
1921.541116	13142.292316	62.532238
1920.881495	13075.372511	62.537242
1920.189373	13020.368793	62.542247
1919.754825	12962.733461	62.547252
1919.097050	12905.474294	62.552257
1918.233698	12864.162325	62.557262
1917.971815	12797.532160	62.562266
1916.674232	12739.713308	62.567271
1916.482100	12676.907929	62.572276
1915.652023	12627.513510	62.577281
1914.985271	12565.222095	62.582286
1914.617524	12505.949556	62.587290
1913.839857	12456.800677	62.592295
1913.521615	12400.917007	62.597300
1912.520947	12325.074247	62.602305
1911.799623	12273.945844	62.607310
1911.221499	12226.095271	62.612314
1910.309873	12154.728591	62.617319
1909.894892	12112.916648	62.622324
1909.285751	12047.372098	62.627329
1908.575940	11979.449538	62.632334
1908.019853	11928.717044	62.637338
1907.458645	11896.324295	62.642343
1907.301425	11810.508830	62.647348
1906.114450	11745.774585	62.652353
1905.182767	11699.875574	62.657358
1904.880058	11623.602007	62.662362
1904.139421	11563.230848	62.667367
1903.542807	11517.320230	62.672372
1902.771206	11450.995859	62.677377
1901.886581	11389.201127	62.682382
1901.262798	11316.661795	62.687386
1900.545620	11297.296836	62.692391
1899.960193	11200.867138	62.697396
1899.339679	11172.535314	62.702401
1898.523247	11106.989676	62.707406
1898.074733	11037.659701	62.712410
1897.091399	11008.521399	62.717415
1896.719061	10930.780972	62.722420
1895.939660	10910.552345	62.727425
1895.811316	10810.872005	62.732430
1894.952168	10786.442632	62.737434
1893.896160	10711.311096	62.742439
1893.642994	10650.840949	62.747444
1893.045228	10595.552347	62.752449
1892.137068	10527.840598	62.757454
1891.525555	10472.243369	62.762458
1890.727484	10418.142715	62.767463
1890.300959	10352.864314	62.772468
1889.249927	10296.999819	62.777473
1888.545058	10247.887210	62.782478
1888.086207	10193.653822	62.787482
1887.141439	10154.092456	62.792487
1886.876444	10089.173002	62.797492
1885.981878	10028.300655	62.802497
1885.469334	9970.838223	62.807502
1884.857507	9916.386722	62.812506
1884.134842	9866.905000	62.817511
1883.725214	9802.806605	62.822516
1883.145496	9753.213015	62.827521
1882.517303	9683.765528	62.832526
1881.795614	9621.628712	62.837530
1881.002411	9571.441210	62.842535
1880.492725	9503.460559	62.847540
1879.808861	9448.718445	62.852545
1878.673644	9386.806440	62.857550
1878.388459	9336.959184	62.862554
1877.519331	9280.552050	62.867559
1876.878294	9213.191981	62.872564
1876.027451	9167.037781	62.877569
1875.485385	9107.719482	62.882574
1875.141962	9054.690388	62.887578
1874.415723	9005.730799	62.892583
1873.958482	8930.478008	62.897588
1872.879384	8875.667805	62.902593
1871.961948	8825.959707	62.907598
1871.752321	8754.327884	62.912602
1871.138778	8709.417830	62.917607
1870.612008	8656.188896	62.922612
1869.523288	8592.986877	62.927617
1869.030399	8540.053944	62.932622
1868.699259	8476.528208	62.937626
1867.441817	8434.514705	62.942631
1866.963440	8368.314777	62.947636
1866.561889	8311.346374	62.952641
1865.645330	8254.781821	62.957646
1864.927944	8203.062747	62.962650
1864.075703	8151.682393	62.967655
1863.961923	8089.089385	62.972660
1862.986159	8036.430546	62.977665
1862.483827	7974.211317	62.982670
1862.073632	7916.059329	62.987674
1861.152499	7853.412476	62.992679
1860.556529	7806.831531	62.997684
1859.909387	7742.635700	63.002689
1859.151787	7684.109058	63.007694
1858.726506	7630.794698	63.012698
1857.497546	7579.977448	63.017703
1857.105075	7514.274903	63.022708
1856.445091	7474.538169	63.027713
1855.683884	7417.153822	63.032718
1855.263350	7358.532347	63.037722
1854.477733	7293.368079	63.042727
1854.077669	7242.916161	63.047732
1853.214302	7178.651390	63.052737
1852.623212	7123.489335	63.057742
1851.891283	7065.310504	63.062746
1851.082676	7002.053021	63.067751
1850.563119	6946.727233	63.072756
1849.685428	6899.227560	63.077761
1849.088188	6832.266092	63.082766
1848.604685	6787.621218	63.087770
1847.671567	6739.549505	63.092775
1846.920578	6677.956528	63.097780
1846.525920	6627.434060	63.102785
1845.882272	6571.735761	63.107790
1845.421301	6512.870049	63.112794
1844.297852	6469.030560	63.117799
1843.984403	6399.324370	63.122804
1842.871134	6352.516974	63.127809
1842.645284	6299.954258	63.132814
1842.247252	6239.640106	63.137818
1841.614968	6189.141875	63.142823
1840.861004	6117.187948	63.147828
1840.230497	6072.089784	63.152833
1839.294936	6011.644209	63.157838
1838.474065	5954.652027	63.162842
1837.543634	5905.729155	63.167847
1837.167954	5848.262061	63.172852
1836.557521	5806.353635	63.177857
1835.961945	5748.159117	63.182862
1835.290859	5686.856515	63.187866
1834.397958	5639.553395	63.192871
1834.105561	5581.516468	63.197876
1832.990175	5530.582933	63.202881
1832.484595	5476.579197	63.207886
1831.916198	5418.891975	63.212890
1831.134902	5369.784721	63.217895
1830.937561	5313.231562	63.222900
1829.897597	5263.714579	63.227905
1829.409726	5209.633289	63.232910
1828.792583	5147.482004	63.237914
1828.046565	5094.071528	63.242919
1827.249583	5044.516702	63.247924
1826.448690	4995.921740	63.252929
1826.159496	4939.279699	63.257934
1825.494863	4880.713887	63.262938
1824.510087	4838.419666	63.267943
1824.148875	4772.148560	63.272948
1823.515700	4720.649900	63.277953
1822.712514	4658.777080	63.282958
1822.256848	4610.035510	63.287962
1821.561821	4554.031193	63.292967
1820.909872	4491.828260	63.297972
1820.257171	4441.337678	63.302977
1819.520835	4387.632474	63.307982
1819.060000	4333.684184	63.312986
1818.155791	4274.464001	63.317991
1817.568130	4228.655657	63.322996
1816.828114	4166.871096	63.328001
1815.935720	4103.450058	63.333006
1815.024987	4060.985435	63.338010
1814.598333	4014.335138	63.343015
1813.983543	3944.998327	63.348020
1813.442807	3910.185317	63.353025
1812.987812	3853.017780	63.358030
1812.423431	3805.543791	63.363034
1811.632012	3744.599620	63.368039
1810.848789	3682.435157	63.373044
1810.208753	3630.863333	63.378049
1809.369447	3575.354114	63.383054
1808.960098	3516.811563	63.388058
1808.407411	3470.918803	63.393063
1807.624555	3407.606410	63.398068
1806.390960	3360.190447	63.403073
1806.052841	3298.800764	63.408078
1805.707802	3256.599586	63.413082
1804.414099	3223.198749	63.418087
1804.067254	3158.875796	63.423092
1803.388420	3112.057066	63.428097
1802.650650	3068.130219	63.433102
1802.291633	3017.905465	63.438106
1801.796003	2963.934617	63.443111
1800.909332	2893.244604	63.448116
1800.280041	2849.090634	63.453121
1799.464799	2805.084614	63.458126
1799.076018	2745.888132	63.463130
1798.030555	2699.494852	63.468135
1797.387129	2647.563493	63.473140
1796.584962	2586.882146	63.478145
1795.944335	2544.395602	63.483150
1795.368455	2497.676838	63.488154
1794.733574	2452.087375	63.493159
1794.389589	2395.283266	63.498164
1793.600540	2356.403336	63.503169
1792.516143	2310.638086	63.508174
1792.432374	2233.779377	63.513178
1791.444985	2187.742824	63.518183
1790.947705	2154.984460	63.523188
1790.093738	2091.420955	63.528193
1789.543819	2047.054150	63.533198
1789.071216	1992.457124	63.538202
1788.264359	1931.503257	63.543207
1788.060080	1879.982759	63.548212
1787.117130	1825.714173	63.553217
1786.382423	1785.990493	63.558222
1785.896513	1718.008745	63.563226
1784.774945	1680.799143	63.568231
1784.108294	1628.729226	63.573236
1783.492926	1588.466704	63.578241
1782.852956	1532.653678	63.583246
1782.287129	1481.358383	63.588250
1781.636465	1442.999063	63.593255
1780.865174	1389.762257	63.598260
1780.377204	1349.797151	63.603265
1779.217024	1287.253303	63.608270
1778.865317	1240.972930	63.613274
1778.084716	1200.002831	63.618279
1777.343890	1152.224861	63.623284
1776.467751	1108.098816	63.628289
1776.089160	1064.029515	63.633294
1775.631809	1001.939066	63.638298
1774.785476	974.821375	63.643303
1774.104215	911.405134	63.648308
1773.311123	885.053459	63.653313
1772.549031	835.355988	63.658318
1772.233453	766.681423	63.663322
1771.323813	748.506195	63.668327
1770.761357	690.938390	63.673332
1769.813097	673.496371	63.678337
1768.982874	618.297400	63.683342
1768.906740	560.359568	63.688346
1767.827342	527.839248	63.693351
1767.649311	508.073693	63.698356
1766.806692	431.282723	63.703361
1766.029339	421.545596	63.708366
1765.704978	347.561714	63.713370
1764.487340	317.585333	63.718375
1763.970902	275.479939	63.723380
1763.100254	228.764827	63.728385
1762.388910	211.643706	63.733390
1762.009532	151.431296	63.738394
1760.782190	116.943768	63.743399
1760.167820	103.924671	63.748404
1759.427086	48.084484	63.753409
1758.780555	28.494909	63.758414
1758.387645	-14.305744	63.763418
1757.525552	-35.398465	63.768423
1756.458776	-80.690612	63.773428
1755.476118	-75.690361	63.778433
1752.423042	-53.838709	63.783438
1748.467575	40.370012	63.788442
1749.159374	39.355017	63.793447
1750.162219	28.144887	63.798452
1751.325023	35.578202	63.803457
1750.974358	44.385670	63.808462
1750.856086	18.623825	63.813466
1749.269865	39.621365	63.818471
1748.129263	37.309450	63.823476
1747.908027	42.037436	63.828481
1746.985564	41.051738	63.833486
1746.357364	48.458850	63.838490
1745.824732	46.532909	63.843495
1744.788292	42.409946	63.848500
1744.206418	57.314151	63.853505
1743.888299	57.225918	63.858510
1743.906938	30.953472	63.863514
1742.702227	62.461955	63.868519
1741.652959	42.392302	63.873524
1741.732897	46.274548	63.878529
1740.694599	57.439886	63.883534
1740.261647	53.020810	63.888538
1739.134337	45.594492	63.893543
1738.959339	35.585361	63.898548
1738.560949	38.458669	63.903553
1737.020633	48.517907	63.908558
1737.055368	35.760053	63.913562
1735.867435	57.468621	63.918567
1735.569989	40.378172	63.923572
1734.877014	41.620452	63.928577
1733.782856	56.725862	63.933582
1733.505458	43.438854	63.938586
1732.902788	52.019855	63.943591
1731.912906	58.893082	63.948596
1731.445483	48.340628	63.953601
1730.956719	52.106624	63.958606
1730.349721	43.651536	63.963610
1729.488449	58.237431	63.968615
1728.675620	42.923999	63.973620
1728.350217	55.789544	63.978625
1727.406225	55.311878	63.983630
1727.298471	44.713342	63.988634
1726.557080	44.198769	63.993639
1726.035352	42.640095	63.998644
1725.007816	40.781725	64.003649
1723.524144	45.386955	64.008654
1723.454441	37.404758	64.013658
1722.895667	48.504972	64.018663
1722.621665	49.366910	64.023668
1722.207983	50.627911	64.028673
1720.531370	50.022188	64.033678
1720.564342	48.006420	64.038682
1719.757519	49.766662	64.043687
1719.168789	38.556998	64.048692
1718.079014	56.523778	64.053697
1717.606975	54.279148	64.058702
1717.753801	44.392359	64.063706
1716.268492	58.427690	64.068711
1715.477908	43.074462	64.073716
1714.753195	45.961759	64.078721
1714.372341	47.840420	64.083726
1713.976203	36.224869	64.088730
1713.015856	52.598926	64.093735
1712.271956	37.361289	64.098740
1712.046442	48.033272	64.103745
1711.103271	38.401609	64.108750
1710.891794	55.142410	64.113754
1710.172795	51.271805	64.118759
1709.299206	48.053358	64.123764
1708.794896	45.050639	64.128769
1708.166790	54.435171	64.133774
1707.954855	42.679977	64.138778
1706.621446	44.145406	64.143783
1705.783764	44.327351	64.148788
1704.744244	47.805527	64.153793
1704.139978	60.232838	64.158798
1703.939471	57.260708	64.163802
1703.422492	57.953091	64.168807
1702.856264	51.891568	64.173812
1702.176967	53.153761	64.178817
1701.518903	55.795519	64.183822
1701.157288	59.016220	64.188826
1700.526392	54.045141	64.193831
1699.373635	53.979100	64.198836
1698.411548	41.458420	64.203841
1697.381668	54.639278	64.208846
1697.226391	48.375294	64.213850
1696.830614	43.120880	64.218855
1696.383462	57.939037	64.223860
1695.518282	52.047997	64.228865
1694.832052	42.129533	64.233870
1694.282625	46.692039	64.238874
1693.698335	51.280584	64.243879
1693.198745	42.455224	64.248884
1691.986742	48.392372	64.253889
1690.751810	54.924500	64.258894
1690.891322	42.411768	64.263898
1690.118808	54.561459	64.268903
1689.398181	44.623229	64.273908
1688.791726	46.179772	64.278913
1688.276535	56.670699	64.283918
1687.818582	45.657879	64.288922
1687.283652	55.005537	64.293927
1686.678940	43.375811	64.298932
1685.912937	38.863002	64.303937
1684.345794	44.478107	64.308942
1684.090168	43.698737	64.313946
1683.188078	57.201489	64.318951
1682.858139	36.103023	64.323956
1682.475946	32.066974	64.328961
1681.762025	42.463306	64.333966
1681.601554	49.064455	64.338970
1680.911988	42.440659	64.343975
1680.108933	38.835721	64.348980
1679.514445	41.576189	64.353985
1678.298410	51.317452	64.358990
1678.037754	42.026806	64.363994
1676.389869	49.001409	64.368999
1675.768424	46.649639	64.374004
1675.562487	47.620613	64.379009
1674.933919	41.160589	64.384014
1674.607597	38.832902	64.389018
1673.722074	45.337916	64.394023
1673.088429	50.309604	64.399028
1672.806318	43.110175	64.404033
1672.075688	50.326996	64.409038
1671.313131	46.923777	64.414042
1670.244225	46.249940	64.419047
1669.354151	42.923745	64.424052
1668.996881	44.655168	64.429057
1668.252283	47.603980	64.434062
1668.284936	44.812432	64.439066
1667.427438	50.524552	64.444071
1666.768710	41.377562	64.449076
1665.868397	38.693215	64.454081
1664.940314	50.146978	64.459086
1664.723078	35.967377	64.464090
1663.919158	40.026283	64.469095
1663.308347	53.318769	64.474100
1662.831508	44.343152	64.479105
1661.848299	48.682843	64.484110
1660.983055	33.899732	64.489114
1660.334657	33.365675	64.494119
1659.503456	49.610419	64.499124
1659.388394	45.200789	64.504129
1658.668113	46.780151	64.509134
1658.538710	36.776406	64.514138
1657.504978	41.330695	64.519143
1656.563797	53.463031	64.524148
1656.340809	42.430244	64.529153
1655.677841	42.890369	64.534158
1654.520409	59.163292	64.539162
1653.458479	30.725564	64.544167
1652.665977	48.009639	64.549172
1652.779145	38.721116	64.554177
1652.141605	32.350834	64.559182
1651.610997	45.288388	64.564186
1651.087975	36.801068	64.569191
1650.104266	35.192801	64.574196
1648.796775	49.141559	64.579201
1648.121667	43.212464	64.584206
1648.422395	35.376429	64.589210
1647.164325	28.491313	64.594215
1646.570246	45.105223	64.599220
1646.132226	40.116142	64.604225
1645.510208	39.458054	64.609230
1645.236833	38.355091	64.614234
1644.403336	47.035846	64.619239
1643.236386	32.540360	64.624244
1642.634556	46.641938	64.629249
1641.903888	47.945420	64.634254
1641.827138	38.909410	64.639258
1641.216133	45.809200	64.644263
1640.228535	37.160726	64.649268
1639.156496	34.763857	64.654273
1638.487946	43.185028	64.659278
1638.185639	32.541730	64.664282
1637.639535	44.201309	64.669287
1637.176333	53.195392	64.674292
1636.197110	27.552993	64.679297
1635.114858	46.887327	64.684302
1634.826969	38.003126	64.689306
1634.349493	45.665420	64.694311
1633.718178	39.303613	64.699316
1633.530140	34.358400	64.704321
1631.879666	44.807332	64.709326
1631.260865	26.952727	64.714330
1630.329366	45.170325	64.719335
1630.180126	40.430250	64.724340
1630.052838	40.302254	64.729345
1629.176764	32.295213	64.734350
1628.606947	42.684431	64.739354
1627.449204	49.830346	64.744359
1626.772505	37.776860	64.749364
1626.373255	29.396040	64.754369
1625.504218	44.910385	64.759374
1625.564089	37.494219	64.764378
1624.517653	36.209729	64.769383
1623.595502	40.951300	64.774388
1622.811794	37.713878	64.779393
1622.036838	47.298359	64.784398
1621.967249	28.050839	64.789402
1621.290551	26.590923	64.794407
1619.978788	33.759725	64.799412
1619.298715	37.428398	64.804417
1618.838835	47.066899	64.809422
1618.737342	37.672138	64.814426
1617.875070	44.868882	64.819431
1617.383963	29.192183	64.824436
1616.269734	30.145037	64.829441
1615.219441	45.984636	64.834446
1615.024871	35.455109	64.839450
1614.672354	34.539757	64.844455
1614.013370	31.747709	64.849460
1613.353309	49.837041	64.854465
1612.539995	46.845589	64.859470
1611.922318	33.008730	64.864474
1611.243520	41.012079	64.869479
1610.758077	39.758314	64.874484
1609.857694	47.661256	64.879489
1608.876824	47.159532	64.884494
1608.319372	40.178895	64.889498
1607.997046	46.933484	64.894503
1607.262455	37.692919	64.899508
1606.762583	40.941897	64.904513
1605.219070	46.237913	64.909518
1604.957962	42.188947	64.914522
1604.243827	44.191530	64.919527
1603.856050	40.873867	64.924532
1603.973836	31.981994	64.929537
1602.788118	50.164300	64.934542
1601.707553	40.636514	64.939546
1601.216254	38.374470	64.944551
1600.803385	38.326538	64.949556
1600.492561	38.852152	64.954561
1599.358710	44.291236	64.959566
1599.016621	39.430422	64.964570
1597.929252	44.601935	64.969575
1597.351168	37.291856	64.974580
1596.224554	34.285535	64.979585
1595.296764	44.129256	64.984590
1594.731049	34.855560	64.989594
1594.356681	36.089832	64.994599
1594.029856	39.778080	64.999604
1593.833005	27.783992	65.004609
1593.130406	42.808291	65.009614
1592.764081	37.449878	65.014618
1591.695994	38.308683	65.019623
1590.634108	36.611939	65.024628
1589.869894	32.049997	65.029633
1588.634503	40.018781	65.034638
1588.215493	35.056655	65.039642
1587.660290	44.035392	65.044647
1587.336246	41.049791	65.049652
1587.070495	39.122486	65.054657
1586.371745	45.261971	65.059662
1585.908793	40.477130	65.064666
1584.563755	48.909601	65.069671
1583.950017	42.328981	65.074676
1583.772186	37.538264	65.079681
1583.001362	41.186673	65.084686
1582.251181	43.357408	65.089690
1581.276314	39.018163	65.094695
1580.738991	47.636107	65.099700
1580.585353	40.952428	65.104705
1579.363897	35.379811	65.109710
1578.603384	51.991791	65.114714
1578.144907	44.189643	65.119719
1577.378160	37.363690	65.124724
1577.367718	39.013212	65.129729
1576.036859	39.743468	65.134734
1575.299278	40.876185	65.139738
1574.442688	38.006737	65.144743
1574.073553	38.223087	65.149748
1573.974743	37.847727	65.154753
1573.117505	45.901513	65.159758
1572.412788	33.880886	65.164762
1571.375957	37.886939	65.169767
1570.930219	27.575521	65.174772
1570.644711	37.011279	65.179777
1569.171564	50.488088	65.184782
1568.545316	39.382205	65.189786
1568.027566	43.241134	65.194791
1567.721377	31.890446	65.199796
1567.194556	32.122388	65.204801
1566.475289	43.435762	65.209806
1566.121264	29.476613	65.214810
1565.239636	44.770627	65.219815
1564.356386	37.706156	65.224820
1563.418405	24.834813	65.229825
1562.127099	42.787902	65.234830
1561.817108	37.217124	65.239834
1561.175069	37.675524	65.244839
1560.628951	31.189825	65.249844
1560.704333	38.710667	65.254849
1559.946593	45.067680	65.259854
1559.779900	38.963221	65.264858
1558.887706	39.297372	65.269863
1558.237849	38.590115	65.274868
1557.319563	34.415350	65.279873
1556.027411	46.907807	65.284878
1555.387089	34.876955	65.289882
1555.026114	40.801934	65.294887
1554.659398	40.532218	65.299892
1554.232956	33.954967	65.304897
1552.888115	38.208655	65.309902
1552.593523	31.056967	65.314906
1551.907334	42.005555	65.319911
1551.067688	39.743680	65.324916
1550.542111	33.221605	65.329921
1549.645608	40.795949	65.334926
1549.121719	39.171429	65.339930
1548.495537	41.754539	65.344935
1547.534018	48.576003	65.349940
1547.044002	35.972512	65.354945
1546.333971	43.995028	65.359950
1546.109970	40.979346	65.364954
1545.731690	39.030504	65.369959
1544.390641	35.181527	65.374964
1543.843576	42.020711	65.379969
1543.143316	45.810877	65.384974
1542.652598	26.849481	65.389978
1541.852588	39.076089	65.394983
1540.999084	38.667690	65.399988
1540.589946	32.617529	65.404993
1539.731679	39.438354	65.409998
1539.464233	32.149896	65.415002
1538.456157	40.114118	65.420007
1537.463855	39.081249	65.425012
1537.146888	45.406075	65.430017
1536.462749	43.434873	65.435022
1536.392043	34.024196	65.440026
1535.649067	36.824554	65.445031
1534.555560	37.772573	65.450036
1533.962607	32.298803	65.455041
1533.527663	35.597397	65.460046
1532.648806	33.352798	65.465050
1531.366621	33.570738	65.470055
1530.979034	30.275137	65.475060
1530.658193	35.047338	65.480065
1529.929765	41.289316	65.485070
1529.601730	34.008910	65.490074
1528.554321	37.152523	65.495079
1527.755929	42.705479	65.500084
1527.198593	30.461190	65.505089
1526.567111	43.085209	65.510094
1526.526881	27.212326	65.515098
1525.351994	29.352794	65.520103
1524.571671	32.991686	65.525108
1524.320185	38.170744	65.530113
1523.503035	41.162658	65.535118
1523.150770	34.013832	65.540122
1521.992273	37.419517	65.545127
1521.474552	39.014033	65.550132
1521.123502	26.930927	65.555137
1519.934004	36.387334	65.560142
1519.167612	30.753479	65.565146
1518.674515	40.963364	65.570151
1518.243204	39.451868	65.575156
1517.624385	36.051091	65.580161
1516.713769	43.615073	65.585166
1515.755526	30.295979	65.590170
1515.047340	34.522630	65.595175
1514.668562	42.763738	65.600180
1514.539440	30.066647	65.605185
1513.554888	30.576332	65.610190
1512.756072	26.355795	65.615194
1512.248147	38.595916	65.620199
1511.665033	43.171687	65.625204
1510.879521	31.837259	65.630209
1509.625619	44.096581	65.635214
1509.070251	48.213801	65.640218
1508.526887	37.247728	65.645223
1508.123291	33.491069	65.650228
1507.624825	34.525885	65.655233
1507.088054	40.253306	65.660238
1506.258134	35.451108	65.665242
1505.150677	42.999066	65.670247
1504.756871	37.451080	65.675252
1504.564343	37.095347	65.680257
1503.827303	49.769262	65.685262
1502.884360	35.733406	65.690266
1502.253135	38.208521	65.695271
1501.765495	41.480803	65.700276
1501.270630	33.372239	65.705281
1500.021654	45.121447	65.710286
1499.721188	35.256872	65.715290
1498.861525	42.092123	65.720295
1498.327818	44.468168	65.725300
1497.585487	43.498089	65.730305
1496.464935	45.558977	65.735310
1495.982259	38.238497	65.740314
1495.632347	43.759616	65.745319
1495.117003	36.939472	65.750324
1495.136420	29.332635	65.755329
1493.691705	42.492727	65.760334
1493.208103	38.452328	65.765338
1492.606997	40.637242	65.770343
1491.344524	41.321983	65.775348
1490.749295	33.994163	65.780353
1490.100566	42.606165	65.785358
1489.672244	32.977946	65.790362
1489.041632	43.917713	65.795367
1488.755519	34.672154	65.800372
1487.932713	37.865242	65.805377
1486.883260	48.302315	65.810382
1486.660735	37.613256	65.815386
1485.678819	40.631365	65.820391
1485.092411	41.683315	65.825396
1484.597047	26.358990	65.830401
1483.982352	42.367502	65.835406
1482.867667	38.805849	65.840410
1481.967481	47.036786	65.845415
1481.373787	41.165768	65.850420
1481.081280	34.810091	65.855425
1480.722162	45.031806	65.860430
1480.305338	39.733476	65.865434
1479.081086	42.835829	65.870439
1478.318531	40.415078	65.875444
1478.129128	37.240948	65.880449
1477.192694	47.100266	65.885454
1476.221917	32.723511	65.890458
1475.611151	29.189010	65.895463
1474.761598	40.776980	65.900468
1474.641306	30.885357	65.905473
1474.132728	42.461717	65.910478
1473.395127	41.342666	65.915482
1472.513264	44.849484	65.920487
1472.078012	37.122521	65.925492
1471.431485	38.806900	65.930497
1470.118446	50.660917	65.935502
1469.769925	39.908309	65.940506
1469.032354	51.182036	65.945511
1468.572565	44.679484	65.950516
1468.527252	34.679753	65.955521
1467.589367	40.015205	65.960526
1466.495867	28.121066	65.965530
1466.176568	47.523410	65.970535
1465.443022	24.201115	65.975540
1464.960946	32.881243	65.980545
1463.513416	51.400073	65.985550
1463.437708	42.187306	65.990554
1462.973382	43.207244	65.995559
1461.846710	41.320585	66.000564
1461.172993	48.928934	66.005569
1460.504312	55.730695	66.010574
1460.294820	47.065869	66.015578
1459.136798	40.002533	66.020583
1458.400593	46.811868	66.025588
1458.141388	35.340201	66.030593
1457.445177	41.709533	66.035598
1457.294173	39.308286	66.040602
1456.310812	50.411352	66.045607
1455.255646	33.279000	66.050612
1454.757627	30.202805	66.055617
1453.787440	55.476863	66.060622
1453.197190	32.790928	66.065626
1452.261700	31.553530	66.070631
1451.946768	51.207486	66.075636
1451.767570	36.346981	66.080641
1450.978045	50.833208	66.085646
1450.298632	39.246980	66.090650
1449.641124	29.820772	66.095655
1449.069673	58.046475	66.100660
1448.189687	29.179452	66.105665
1447.098015	48.233060	66.110670
1446.917223	41.377102	66.115674
1446.330571	32.507313	66.120679
1445.376208	45.054929	66.125684
1444.724704	36.487169	66.130689
1443.804113	37.563856	66.135694
1443.630804	39.838479	66.140698
1443.473769	34.197685	66.145703
1442.070891	39.342130	66.150708
1441.370656	44.490017	66.155713
1440.596227	42.392849	66.160718
1440.297657	36.675206	66.165722
1439.893915	37.163568	66.170727
1438.624284	43.218780	66.175732
1438.246978	37.139927	66.180737
1437.634694	46.082025	66.185742
1436.945540	40.674029	66.190746
1435.900433	37.047726	66.195751
1435.180316	33.306696	66.200756
1434.883417	36.854588	66.205761
1434.294218	36.260720	66.210766
1433.789511	35.372737	66.215770
1432.741454	41.832687	66.220775
1431.928256	36.550061	66.225780
1431.833095	38.239853	66.230785
1431.587427	34.853907	66.235790
1430.544717	39.436509	66.240794
1429.557332	34.602599	66.245799
1428.853904	44.683505	66.250804
1428.705428	27.340839	66.255809
1427.356227	36.937775	66.260814
1426.817955	33.626720	66.265818
1426.209346	40.795809	66.270823
1425.643057	39.025096	66.275828
1425.093962	34.763321	66.280833
1423.974018	38.650178	66.285838
1423.677453	40.487094	66.290842
1423.284943	43.868842	66.295847
1422.545024	39.233712	66.300852
1421.308171	28.103520	66.305857
1420.940116	45.277580	66.310862
1420.607219	33.980055	66.315866
1420.049631	40.138134	66.320871
1419.118851	42.641957	66.325876
1418.569779	32.805878	66.330881
1417.422410	38.649284	66.335886
1417.307255	43.371458	66.340890
1416.608584	44.479112	66.345895
1415.841881	43.284282	66.350900
1415.171634	33.571538	66.355905
1414.750643	38.608815	66.360910
1413.326851	43.024923	66.365914
1412.901420	41.779005	66.370919
1412.041229	50.225946	66.375924
1412.013853	38.496675	66.380929
1411.538885	48.464006	66.385934
1410.534674	38.334429	66.390938
1409.858020	33.410140	66.395943
1409.081543	39.642434	66.400948
1408.636807	32.953013	66.405953
1407.330198	45.260172	66.410958
1407.136306	30.439865	66.415962
1406.193078	43.876661	66.420967
1405.766632	49.162381	66.425972
1405.559320	42.900401	66.430977
1405.149232	44.479408	66.435982
1404.343749	43.871041	66.440986
1403.430224	41.466425	66.445991
1402.364571	40.841068	66.450996
1401.597578	46.403258	66.456001
1400.734968	58.620935	66.461006
1400.711822	41.106957	66.466010
1400.333203	42.755076	66.471015
1399.081392	37.854403	66.476020
1398.496547	38.333713	66.481025
1397.874595	50.410632	66.486030
1397.454363	38.880997	66.491034
1396.639695	38.001291	66.496039
1395.647206	38.788237	66.501044
1395.519148	33.954941	66.506049
1395.086539	46.148412	66.511054
1394.332926	37.697820	66.516058
1393.273675	46.072330	66.521063
1392.691564	46.164868	66.526068
1392.170112	34.928859	66.531073
1390.843819	39.485591	66.536078
1390.355276	38.519358	66.541082
1389.794590	36.538037	66.546087
1389.358628	43.301237	66.551092
1388.944773	38.883937	66.556097
1387.683505	32.354274	66.561102
1387.127952	39.347785	66.566106
1386.715969	39.541010	66.571111
1386.359410	30.754510	66.576116
1385.940870	36.548306	66.581121
1384.885755	36.894221	66.586126
1384.297412	40.904743	66.591130
1383.316271	46.324366	66.596135
1382.116644	33.245550	66.601140
1381.876283	31.870876	66.606145
1381.418819	42.740556	66.611150
1381.056419	37.867243	66.616154
1380.763652	33.470121	66.621159
1379.167413	33.205070	66.626164
1378.778353	26.590384	66.631169
1377.825967	33.123446	66.636174
1377.505712	36.919473	66.641178
1376.676457	45.924451	66.646183
1375.857138	38.643324	66.651188
1375.777114	32.329582	66.656193
1375.307487	44.306595	66.661198
1374.341367	36.359705	66.666202
1373.567050	34.041778	66.671207
1372.900038	34.614576	66.676212
1372.785348	41.785582	66.681217
1371.543175	36.914930	66.686222
1371.063777	34.591123	66.691226
1370.083686	35.462837	66.696231
1368.985180	37.286892	66.701236
1368.505868	34.225089	66.706241
1367.976500	40.082235	66.711246
1367.520007	30.338686	66.716250
1367.356860	29.134659	66.721255
1366.433222	34.988248	66.726260
1365.675654	37.106601	66.731265
1365.053191	35.305410	66.736270
1364.291550	40.508803	66.741274
1363.584049	34.950792	66.746279
1362.980979	38.482707	66.751284
1362.616140	35.520975	66.756289
1361.508165	41.865899	66.761294
1360.808170	36.111161	66.766298
1360.142567	38.979687	66.771303
1359.503745	43.414536	66.776308
1359.389057	30.149077	66.781313
1358.329932	37.497020	66.786318
1357.699962	31.010516	66.791322
1357.121872	34.532153	66.796327
1356.310936	32.696274	66.801332
1355.627985	33.998554	66.806337
1354.904228	45.084027	66.811342
1354.107397	36.768050	66.816346
1353.968704	36.334388	66.821351
1352.986534	38.062688	66.826356
1352.502086	29.854746	66.831361
1351.491279	35.950845	66.836366
1351.288877	29.812673	66.841370
1350.628103	37.825814	66.846375
1349.597476	36.795959	66.851380
1349.013188	36.748510	66.856385
1348.507271	38.785864	66.861390
1347.994483	33.887582	66.866394
1347.251006	35.254678	66.871399
1346.670544	36.241060	66.876404
1345.925168	29.965287	66.881409
1344.782076	41.391798	66.886414
1343.991035	39.880752	66.891418
1343.790330	33.046902	66.896423
1343.091818	41.291541	66.901428
1342.702775	33.568306	66.906433
1341.633451	42.933140	66.911438
1340.839190	32.697689	66.916442
1340.665198	36.202395	66.921447
1339.884569	41.257432	66.926452
1339.154192	30.898291	66.931457
1338.384643	33.428546	66.936462
1337.960042	39.948679	66.941466
1337.437822	38.869543	66.946471
1336.530864	43.294987	66.951476
1335.879260	34.422942	66.956481
1334.815540	34.136337	66.961486
1334.424680	32.919630	66.966490
1334.154721	30.050048	66.971495
1332.863314	27.819071	66.976500
1332.704347	30.876706	66.981505
1331.836058	49.864867	66.986510
1331.406447	32.410801	66.991514
1330.753412	28.843637	66.996519
1329.715122	33.453954	67.001524
1329.926607	31.564348	67.006529
1328.794878	42.082349	67.011534
1327.830415	30.882101	67.016538
1327.608142	33.840996	67.021543
1326.455096	39.513459	67.026548
1325.714440	28.730200	67.031553
1324.627202	35.697862	67.036558
1324.345226	33.719555	67.041562
1323.946823	31.586301	67.046567
1323.671498	44.932703	67.051572
1323.245631	24.322702	67.056577
1321.851976	32.824504	67.061582
1321.429102	27.512984	67.066586
1321.139171	36.977831	67.071591
1319.710846	31.755196	67.076596
1318.980696	40.419590	67.081601
1318.557086	34.378087	67.086606
1317.884279	25.550425	67.091610
1317.855120	33.904683	67.096615
1316.535291	40.896713	67.101620
1316.037094	40.709434	67.106625
1315.362563	36.369862	67.111630
1315.070609	33.431242	67.116634
1313.893883	36.116120	67.121639
1313.131515	31.076185	67.126644
1312.968843	27.393222	67.131649
1312.343280	38.084633	67.136654
1311.308323	33.518525	67.141658
1310.709842	36.016859	67.146663
1310.101502	47.265333	67.151668
1309.827727	28.569147	67.156673
1308.443869	28.625173	67.161678
1307.701563	27.923219	67.166682
1307.525749	27.437117	67.171687
1306.958267	37.502731	67.176692
1306.721316	28.063328	67.181697
1305.578972	32.652351	67.186702
1304.830695	36.063866	67.191706
1304.410795	30.043855	67.196711
1303.068193	38.286827	67.201716
1302.846952	23.636473	67.206721
1301.992876	33.760265	67.211726
1301.669087	28.928138	67.216730
1301.023214	31.446624	67.221735
1299.895549	30.588329	67.226740
1299.651194	31.147562	67.231745
1299.124399	35.361192	67.236750
1297.858809	32.911671	67.241754
1297.434339	32.608600	67.246759
1296.700951	35.207231	67.251764
1296.607479	33.858096	67.256769
1295.857176	36.079387	67.261774
1294.933221	35.083054	67.266778
1294.481205	43.083518	67.271783
1293.915324	32.841737	67.276788
1292.941647	29.781284	67.281793
1291.985755	44.379129	67.286798
1291.750599	31.020877	67.291802
1291.468202	28.542770	67.296807
1290.310744	41.977382	67.301812
1289.571610	39.095670	67.306817
1289.102961	41.355758	67.311822
1288.206281	29.450923	67.316826
1287.229513	41.043389	67.321831
1286.313622	47.116539	67.326836
1286.476199	31.285567	67.331841
1285.888428	43.114218	67.336846
1285.253281	38.782584	67.341850
1284.689767	32.444802	67.346855
1283.547810	31.150413	67.351860
1283.342051	26.536057	67.356865
1282.068840	31.518041	67.361870
1281.740424	31.292737	67.366874
1281.264189	35.797939	67.371879
1280.601487	42.283400	67.376884
1279.763957	26.925247	67.381889
1278.817706	35.102055	67.386894
1278.757269	26.451420	67.391898
1278.023930	27.268166	67.396903
1276.553708	33.566639	67.401908
1276.408912	37.544502	67.406913
1275.860330	33.410413	67.411918
1275.353567	25.368461	67.416922
1274.376498	31.361453	67.421927
1273.330842	42.201663	67.426932
1273.004747	22.387918	67.431937
1272.986900	28.477542	67.436942
1272.091073	31.541957	67.441946
1271.364595	30.067977	67.446951
1270.397715	50.391675	67.451956
1270.057472	29.113666	67.456961
1268.652999	33.143589	67.461966
1268.442761	37.827264	67.466970
1267.784648	39.929830	67.471975
1267.433303	31.148837	67.476980
1266.757877	27.288798	67.481985
1265.799703	45.616347	67.486990
1265.611593	30.402510	67.491994
1264.416908	20.066772	67.496999
1263.453681	26.879122	67.502004
1262.919648	26.787434	67.507009
1262.434481	39.970083	67.512014
1262.287903	37.382077	67.517018
1261.403027	23.958419	67.522023
1260.427256	11.416513	67.527028
1260.003461	34.414960	67.532033
1259.499692	33.692438	67.537038
1258.147378	29.446463	67.542042
1257.778339	21.505618	67.547047
1256.948346	26.519635	67.552052
1256.786899	9.937578	67.557057
1256.393436	28.481230	67.562062
1255.317202	26.413191	67.567066
1254.758836	24.228118	67.572071
1253.953360	27.416937	67.577076
1253.327576	17.793384	67.582081
1252.214327	25.406993	67.587086
1252.049323	23.509442	67.592090
1251.758437	25.969916	67.597095
1250.536527	26.728744	67.602100
1249.936170	18.228621	67.607105
1249.316567	33.321747	67.612110
1248.386452	32.845207	67.617114
1248.256683	28.959909	67.622119
1246.971020	31.630599	67.627124
1246.447068	21.314369	67.632129
1245.789078	28.343106	67.637134
1245.711503	32.061131	67.642138
1245.402343	26.936542	67.647143
1244.134754	31.980725	67.652148
1243.676122	26.728523	67.657153
1242.927527	34.227389	67.662158
1242.103709	33.737103	67.667162
1241.765843	26.921928	67.672167
1240.879405	24.735411	67.677172
1240.035489	26.235196	67.682177
1239.344110	20.129067	67.687182
1238.746041	20.001837	67.692186
1238.322507	20.414533	67.697191
1236.971598	24.262495	67.702196
1236.472850	17.297874	67.707201
1235.728102	25.836869	67.712206
1235.578016	13.750280	67.717210
1235.447597	20.772390	67.722215
1234.356133	22.838219	67.727220
1233.855695	25.259479	67.732225
1233.273279	23.737373	67.737230
1231.956314	15.852657	67.742234
1231.041485	19.634432	67.747239
1230.487805	26.596123	67.752244
1230.389671	13.805868	67.757249
1229.992775	22.805189	67.762254
1228.675036	18.616813	67.767258
1228.142941	10.840674	67.772263
1227.618837	26.248178	67.777268
1226.671463	27.381235	67.782273
1226.002328	18.009002	67.787278
1225.012081	26.546039	67.792282
1224.919012	30.851551	67.797287
1224.461963	31.346846	67.802292
1224.023980	16.574874	67.807297
1222.953104	25.345495	67.812302
1222.090022	26.337423	67.817306
1221.871228	18.710149	67.822311
1221.099751	27.008980	67.827316
1220.166972	17.860015	67.832321
1219.597871	24.727969	67.837326
1219.368069	20.786046	67.842330
1218.696220	19.295511	67.847335
1217.148042	32.623542	67.852340
1216.915029	17.459447	67.857345
1216.511952	27.833220	67.862350
1215.506826	29.923173	67.867354
1214.844387	11.109080	67.872359
1214.153129	26.678778	67.877364
1214.187732	23.256179	67.882369
1213.234764	35.481935	67.887374
1212.195608	23.555646	67.892378
1211.660479	20.474373	67.897383
1211.094834	25.873701	67.902388
1210.747027	28.048353	67.907393
1209.813074	28.212652	67.912398
1209.096457	35.818400	67.917402
1208.583100	22.051851	67.922407
1207.385392	26.955631	67.927412
1206.565065	21.499195	67.932417
1206.214179	25.262259	67.937422
1205.523637	28.051208	67.942426
1205.866276	14.087045	67.947431
1204.658804	32.585113	67.952436
1203.942305	22.102406	67.957441
1203.324093	23.017554	67.962446
1202.096305	23.433579	67.967450
1201.631376	16.794735	67.972455
1200.723025	25.921124	67.977460
1200.526774	19.469777	67.982465
1200.002542	30.275962	67.987470
1199.377141	24.160930	67.992474
1199.059676	21.259501	67.997479
1197.830680	31.608510	68.002484
1197.024896	24.628071	68.007489
1196.393533	25.710885	68.012494
1195.864339	31.060268	68.017498
1195.717434	25.982422	68.022503
1194.399393	25.226986	68.027508
1193.857118	23.794696	68.032513
1193.164385	28.760096	68.037518
1192.617817	18.986777	68.042522
1191.832403	35.035063	68.047527
1191.213495	29.660134	68.052532
1190.858809	25.622961	68.057537
1189.760955	30.480909	68.062542
1188.997938	29.947856	68.067546
1188.578688	18.531677	68.072551
1188.023129	14.362457	68.077556
1187.566000	30.017924	68.082561
1186.159209	36.361547	68.087566
1185.735092	18.717451	68.092570
1185.429147	28.733595	68.097575
1184.753137	30.704990	68.102580
1184.552710	16.382509	68.107585
1183.444202	14.560900	68.112590
1182.569873	20.591191	68.117594
1181.826702	30.894480	68.122599
1180.716125	34.715290	68.127604
1180.277415	16.311884	68.132609
1180.002671	20.534327	68.137614
1179.622240	19.656595	68.142618
1179.376506	14.583434	68.147623
1178.075057	28.532954	68.152628
1177.640679	25.238554	68.157633
1176.700372	19.900556	68.162638
1175.677820	30.270353	68.167642
1175.188903	21.746222	68.172647
1174.524827	34.798059	68.177652
1174.695559	26.225784	68.182657
1173.271795	29.399421	68.187662
1172.612585	25.191496	68.192666
1172.182850	20.456666	68.197671
1171.562807	22.505891	68.202676
1170.649206	17.609906	68.207681
1170.007999	26.365826	68.212686
1169.359833	17.204735	68.217690
1168.983436	21.397616	68.222695
1167.736475	19.151775	68.227700
1167.282828	22.205819	68.232705
1166.723914	18.920191	68.237710
1166.205221	24.621127	68.242714
1165.976068	14.882489	68.247719
1164.569900	34.228996	68.252724
1163.977398	12.548066	68.257729
1163.664936	23.847248	68.262734
1163.083351	27.088790	68.267738
1161.975026	25.871106	68.272743
1161.517405	25.075035	68.277748
1161.199629	26.489590	68.282753
1159.979047	28.933937	68.287758
1159.417847	32.869221	68.292762
1158.940600	17.890635	68.297767
1158.447491	28.803831	68.302772
1157.817321	37.628964	68.307777
1156.998234	36.314820	68.312782
1156.605897	30.678372	68.317786
1155.426032	24.085437	68.322791
1154.692416	32.507568	68.327796
1154.108106	23.229095	68.332801
1153.576893	28.171968	68.337806
1152.990444	30.804033	68.342810
1152.243611	24.621600	68.347815
1151.587042	31.415173	68.352820
1151.123722	23.219699	68.357825
1150.427154	31.847241	68.362830
1149.357208	20.275954	68.367834
1149.020032	15.860709	68.372839
1148.050534	27.209203	68.377844
1148.263321	8.695892	68.382849
1146.989906	17.738433	68.387854
1146.321688	21.802696	68.392858
1145.759278	25.181534	68.397863
1144.769314	25.501416	68.402868
1144.179115	18.406291	68.407873
1143.400852	17.229157	68.412878
1142.827931	29.127985	68.417882
1142.891702	27.886308	68.422887
1141.808066	30.961712	68.427892
1140.850991	8.096201	68.432897
1140.426668	20.679407	68.437902
1139.577703	33.240282	68.442906
1139.323095	11.407856	68.447911
1138.218590	17.067932	68.452916
1138.058859	14.814755	68.457921
1137.374100	9.360442	68.462926
1136.083425	19.342400	68.467930
1135.564261	27.169053	68.472935
1134.980910	20.274682	68.477940
1135.042563	14.813608	68.482945
1133.633783	22.512108	68.487950
1133.068750	13.240043	68.492954
1132.813180	14.537478	68.497959
1131.208326	27.973902	68.502964
1130.906565	21.933567	68.507969
1130.461415	18.483204	68.512974
1130.093198	30.858808	68.517978
1129.598889	10.338634	68.522983
1128.304118	24.162532	68.527988
1127.651026	15.962562	68.532993
1127.408331	21.893981	68.537998
1126.336989	30.033958	68.543002
1125.779605	24.685534	68.548007
1125.302168	32.445632	68.553012
1124.736711	22.013046	68.558017
1123.979434	34.983523	68.563022
1122.928960	30.104594	68.568026
1122.606872	36.332486	68.573031
1121.925765	34.124390	68.578036
1121.706674	22.864040	68.583041
1120.219617	34.931928	68.588046
1119.564990	37.158548	68.593050
1119.651992	22.973276	68.598055
1118.445525	33.045931	68.603060
1117.565716	26.974543	68.608065
1117.155266	37.202850	68.613070
1116.771563	29.794198	68.618074
1116.504163	29.887201	68.623079
1115.337238	35.760640	68.628084
1114.885365	32.677183	68.633089
1113.837253	24.943726	68.638094
1112.700210	32.586403	68.643098
1112.557291	29.647761	68.648103
1111.768526	39.089459	68.653108
1111.744083	31.693046	68.658113
1110.886752	33.690146	68.663118
1109.596532	30.371050	68.668122
1109.219126	26.443156	68.673127
1108.811415	35.650784	68.678132
1108.333452	33.164386	68.683137
1107.535610	27.324381	68.688142
1106.633889	36.005065	68.693146
1106.471288	26.404072	68.698151
1105.057102	27.273973	68.703156
1104.361681	26.476317	68.708161
1103.767717	34.628675	68.713166
1103.344976	26.431489	68.718170
1103.151590	23.276959	68.723175
1101.902918	27.625943	68.728180
1101.336781	27.031640	68.733185
1100.873574	28.822556	68.738190
1100.256364	35.110008	68.743194
1099.581962	29.095835	68.748199
1098.699544	34.584995	68.753204
1098.336146	21.847989	68.758209
1097.230174	30.231593	68.763214
1096.669897	24.498878	68.768218
1096.185001	18.355223	68.773223
1095.717905	21.736254	68.778228
1095.061292	26.530357	68.783233
1094.388720	23.349554	68.788238
1093.423653	20.525925	68.793242
1092.674780	25.353626	68.798247
1091.967292	24.997842	68.803252
1091.043374	31.594267	68.808257
1090.674242	34.999141	68.813262
1090.245107	39.025390	68.818266
1089.942661	25.502861	68.823271
1088.632990	32.783518	68.828276
1088.328684	19.611359	68.833281
1087.935479	16.829225	68.838286
1086.508691	19.768431	68.843290
1086.057397	33.887092	68.848295
1085.286434	33.902513	68.853300
1084.943916	32.257130	68.858305
1084.556238	35.338539	68.863310
1083.887446	26.508746	68.868314
1083.364253	23.422451	68.873319
1082.190999	29.418326	68.878324
1081.182670	21.776326	68.883329
1080.485865	22.639352	68.888334
1080.241367	39.467319	68.893338
1080.034759	33.515926	68.898343
1078.772049	27.915453	68.903348
1078.448615	25.207371	68.908353
1077.684624	19.671065	68.913358
1077.096476	35.265381	68.918362
1076.414091	30.389418	68.923367
1075.371390	34.078052	68.928372
1074.705270	24.979767	68.933377
1074.193262	23.550574	68.938382
1074.144716	29.187774	68.943386
1073.303768	37.638037	68.948391
1072.695705	32.728175	68.953396
1071.730242	20.843856	68.958401
1070.742915	27.256416	68.963406
1070.415991	24.917881	68.968410
1070.231830	23.318269	68.973415
1068.726531	28.624260	68.978420
1068.135908	20.818052	68.983425
1067.676471	22.013888	68.988430
1066.924202	40.237749	68.993434
1066.830014	27.227698	68.998439
1065.741475	35.551775	69.003444
1065.138858	21.203415	69.008449
1064.738725	28.402466	69.013454
1063.599913	28.211495	69.018458
1062.839152	30.275247	69.023463
1062.227958	35.743346	69.028468
1062.172258	33.057327	69.033473
1061.610746	30.033899	69.038478
1060.429053	26.221347	69.043482
1059.651857	28.480093	69.048487
1059.217107	29.413396	69.053492
1058.069799	34.746019	69.058497
1057.534837	34.801172	69.063502
1056.897916	37.242599	69.068506
1056.838998	35.107423	69.073511
1055.874959	37.312320	69.078516
1055.329119	19.857938	69.083521
1054.436211	32.397434	69.088526
1053.929226	31.511470	69.093530
1053.687298	30.293193	69.098535
1052.375079	26.501410	69.103540
1051.780270	21.436492	69.108545
1051.402541	31.844088	69.113550
1050.411901	26.805871	69.118554
1050.043402	26.325211	69.123559
1048.900309	39.607805	69.128564
1048.584548	35.892455	69.133569
1048.188431	22.241346	69.138574
1047.474199	29.362640	69.143578
1046.765443	22.628588	69.148583
1045.588233	32.620924	69.153588
1044.980124	27.968111	69.158593
1044.044315	20.295670	69.163598
1043.302576	35.124406	69.168602
1043.329611	30.122978	69.173607
1042.630715	34.449180	69.178612
1042.474489	27.056395	69.183617
1041.392743	29.090796	69.188622
1040.765354	31.421904	69.193626
1040.591653	30.727338	69.198631
1039.287359	34.903859	69.203636
1038.642137	32.122402	69.208641
1038.350584	20.819985	69.213646
1037.157343	23.064504	69.218650
1036.461210	31.288315	69.223655
1035.535988	33.009248	69.228660
1035.288005	31.123339	69.233665
1034.929217	29.592511	69.238670
1034.257141	32.911551	69.243674
1033.336332	24.260636	69.248679
1032.549180	33.799856	69.253684
1032.269247	30.258574	69.258689
1031.877911	28.600467	69.263694
1030.829386	39.154209	69.268698
1030.643034	31.682641	69.273703
1029.347534	39.369484	69.278708
1028.504791	30.557922	69.283713
1027.997083	24.731711	69.288718
1027.521122	30.768053	69.293722
1026.702066	37.391970	69.298727
1025.659341	37.363916	69.303732
1025.597884	29.825174	69.308737
1025.552549	25.057603	69.313742
1024.018460	29.606564	69.318746
1023.457624	17.143836	69.323751
1022.631606	17.661598	69.328756
1022.326479	30.071318	69.333761
1021.213225	29.400082	69.338766
1020.597591	31.369796	69.343770
1020.358885	23.504459	69.348775
1019.776646	23.713792	69.353780
1018.952178	26.863123	69.358785
1018.104444	35.601469	69.363790
1017.369806	34.318089	69.368794
1017.135828	23.626229	69.373799
1015.813175	26.906859	69.378804
1015.382761	19.627087	69.383809
1014.908182	24.255055	69.388814
1014.537521	27.196576	69.393818
1013.723674	27.900054	69.398823
1013.163552	38.525900	69.403828
1012.598777	29.009406	69.408833
1011.433117	26.274492	69.413838
1010.132615	23.890600	69.418842
1010.232782	26.749327	69.423847
1009.680313	37.545835	69.428852
1009.225954	18.366001	69.433857
1008.455339	29.019023	69.438862
1007.457807	33.662392	69.443866
1007.155064	27.675848	69.448871
1006.425383	35.660588	69.453876
1005.669629	29.383436	69.458881
1005.086398	28.717761	69.463886
1004.313672	30.862277	69.468890
1003.734804	22.978527	69.473895
1002.859826	29.873105	69.478900
1002.576193	30.794989	69.483905
1001.957538	30.052953	69.488910
1000.787923	31.593596	69.493914
1000.013486	24.624016	69.498919
999.509570	32.992286	69.503924
999.249367	39.833209	69.508929
998.804577	26.604575	69.513934
997.598618	37.519250	69.518938
997.318658	34.745918	69.523943
996.272250	27.043785	69.528948
995.271457	28.109735	69.533953
994.566025	35.294295	69.538958
994.019530	35.898474	69.543962
993.949528	33.296732	69.548967
993.384952	27.309274	69.553972
992.637946	22.101439	69.558977
991.535204	26.266412	69.563982
991.174564	24.008944	69.568986
990.658639	23.428754	69.573991
989.571620	26.660866	69.578996
989.264634	19.749375	69.584001
988.934091	25.663240	69.589006
988.104726	33.425734	69.594010
986.887028	27.662039	69.599015
986.431099	30.137759	69.604020
985.882818	24.844692	69.609025
985.675692	24.844545	69.614030
984.377849	25.604542	69.619034
984.105071	24.350183	69.624039
983.235940	22.577305	69.629044
982.432405	32.040297	69.634049
982.021610	21.769223	69.639054
981.037144	34.715948	69.644058
980.325833	21.876646	69.649063
979.028974	32.963476	69.654068
978.589924	25.970500	69.659073
978.688692	21.025470	69.664078
978.009974	37.916209	69.669082
977.807562	28.319994	69.674087
976.565684	30.290019	69.679092
975.994005	22.816700	69.684097
975.311917	23.207503	69.689102
974.866122	25.834568	69.694106
973.979652	31.267639	69.699111
973.110347	29.237760	69.704116
972.763682	18.239007	69.709121
972.067121	26.371436	69.714126
971.306297	33.011328	69.719130
970.521570	27.058907	69.724135
970.089046	26.285686	69.729140
969.480269	21.923149	69.734145
968.908774	29.045400	69.739150
968.186374	25.071509	69.744154
967.082257	21.115782	69.749159
966.155648	26.271402	69.754164
965.776406	19.552754	69.759169
965.469293	27.126499	69.764174
964.584356	35.889701	69.769178
964.639031	29.770601	69.774183
963.569029	26.069631	69.779188
963.148875	22.653170	69.784193
961.935172	27.859205	69.789198
960.795454	30.964103	69.794202
960.556266	29.553022	69.799207
960.262997	28.525843	69.804212
959.855586	26.822999	69.809217
958.956531	31.083302	69.814222
957.928236	31.603311	69.819226
957.578802	29.184801	69.824231
956.491458	28.367552	69.829236
955.884712	30.905119	69.834241
955.415438	30.279668	69.839246
954.812466	37.610352	69.844250
954.311447	25.158622	69.849255
953.459377	27.481349	69.854260
952.732470	37.256994	69.859265
952.586193	20.511744	69.864270
951.520515	32.646691	69.869274
950.598016	28.026586	69.874279
950.278308	26.316097	69.879284
949.528359	30.254645	69.884289
948.694720	35.586282	69.889294
948.003400	29.168017	69.894298
947.608415	19.815336	69.899303
947.156933	36.756645	69.904308
946.318632	36.819092	69.909313
945.582944	35.862315	69.914318
944.751703	31.420070	69.919322
944.257654	20.203513	69.924327
943.276318	36.850686	69.929332
942.616470	33.447139	69.934337
942.690292	16.837175	69.939342
941.900142	36.651833	69.944346
940.979709	27.765944	69.949351
939.972281	27.147288	69.954356
939.784645	27.375844	69.959361
939.232642	27.392735	69.964366
938.018456	29.948124	69.969370
937.833858	19.399807	69.974375
936.860747	29.831188	69.979380
936.316285	34.501828	69.984385
935.610356	25.603885	69.989390
934.985709	33.168243	69.994394
934.689334	35.077712	69.999399
933.772848	26.463999	70.004404
932.814060	30.063641	70.009409
932.318898	29.248357	70.014414
931.714900	31.493770	70.019418
931.184726	26.901125	70.024423
930.437875	28.158491	70.029428
929.948056	26.672184	70.034433
929.057190	32.413460	70.039438
928.060473	19.406721	70.044442
927.612538	17.480109	70.049447
927.194921	26.449632	70.054452
926.605670	23.681378	70.059457
925.627572	25.729292	70.064462
924.767358	28.310355	70.069466
924.447328	21.620138	70.074471
923.228687	28.656154	70.079476
922.659279	29.202496	70.084481
922.298403	23.874894	70.089486
921.641641	24.599133	70.094490
921.763415	24.265967	70.099495
920.642261	23.225467	70.104500
920.153411	26.502758	70.109505
919.447465	25.172267	70.114510
918.070645	26.107285	70.119514
917.817684	20.355677	70.124519
917.036159	31.023068	70.129524
916.718190	32.357260	70.134529
915.619577	24.403292	70.139534
914.807936	33.779284	70.144538
914.135805	25.725909	70.149543
913.810010	26.574090	70.154548
913.367915	19.576887	70.159553
912.756726	11.844966	70.164558
911.749248	27.679473	70.169562
911.548110	18.776901	70.174567
910.529809	22.611513	70.179572
909.570432	22.412557	70.184577
908.819750	23.478159	70.189582
908.428902	22.856005	70.194586
908.383125	16.968931	70.199591
907.193530	28.387205	70.204596
906.626439	23.054579	70.209601
906.594989	18.931329	70.214606
905.190127	24.260844	70.219610
904.382558	21.385421	70.224615
903.754893	33.737667	70.229620
903.315002	13.570030	70.234625
902.863132	25.140544	70.239630
901.773236	27.619402	70.244634
901.365465	14.378612	70.249639
900.472185	30.237526	70.254644
900.339310	25.392436	70.259649
899.496332	24.332906	70.264654
898.430607	33.460769	70.269658
897.949491	25.140468	70.274663
897.061094	28.694229	70.279668
896.317851	27.238799	70.284673
895.749515	23.863280	70.289678
895.411096	38.965304	70.294682
895.099762	16.736724	70.299687
893.893141	20.779500	70.304692
893.185374	29.825164	70.309697
893.036920	28.834869	70.314702
892.017730	26.816258	70.319706
891.353770	20.141362	70.324711
890.638488	31.947761	70.329716
890.185190	24.750504	70.334721
890.023467	25.342352	70.339726
888.668221	36.036407	70.344730
888.178211	17.778463	70.349735
887.351266	28.358474	70.354740
886.306165	29.847814	70.359745
885.756921	23.544150	70.364750
885.415511	20.984033	70.369754
885.136909	28.241024	70.374759
883.991529	39.664892	70.379764
883.151873	27.552494	70.384769
882.917938	30.123780	70.389774
882.358087	31.267824	70.394778
881.798868	21.577038	70.399783
880.511404	28.494720	70.404788
879.921749	37.761280	70.409793
879.734205	28.096489	70.414798
878.847565	21.758220	70.419802
878.261284	13.572935	70.424807
877.423889	30.198782	70.429812
877.141633	33.135710	70.434817
876.305938	28.670548	70.439822
875.147988	44.434416	70.444826
874.899446	24.699924	70.449831
874.468717	37.724120	70.454836
873.662131	29.933418	70.459841
872.882488	31.957652	70.464846
872.288094	36.106419	70.469850
871.392257	24.018740	70.474855
870.642470	31.457952	70.479860
869.927201	24.885840	70.484865
869.777199	22.574369	70.489870
869.252662	30.804014	70.494874
868.639477	14.052683	70.499879
867.697170	27.954615	70.504884
867.062981	29.454253	70.509889
866.324637	23.297381	70.514894
865.495301	36.465438	70.519898
865.222014	23.381435	70.524903
864.379559	31.740525	70.529908
863.423535	35.599937	70.534913
863.066405	31.012881	70.539918
862.567319	27.884957	70.544922
861.871185	22.020975	70.549927
860.680520	31.972942	70.554932
859.734092	29.975879	70.559937
859.717620	25.402412	70.564942
859.049384	32.857031	70.569946
858.445609	24.144700	70.574951
857.509557	29.912110	70.579956
856.794723	32.664012	70.584961
856.977093	21.927997	70.589966
855.772370	22.375208	70.594970
855.444784	31.087570	70.599975
854.576482	39.189018	70.604980
853.616759	30.236885	70.609985
852.693840	27.269458	70.614990
851.976289	39.115651	70.619994
851.656032	31.799459	70.624999
851.442689	31.652085	70.630004
850.488136	28.481545	70.635009
849.974619	26.300470	70.640014
849.175992	35.072039	70.645018
848.352603	22.102405	70.650023
847.314732	22.970896	70.655028
846.826555	20.688023	70.660033
846.656982	29.550268	70.665038
845.901332	30.028504	70.670042
845.465693	20.997695	70.675047
844.631803	30.147017	70.680052
844.190037	25.466211	70.685057
843.256317	24.145190	70.690062
842.240748	27.086880	70.695066
841.896990	18.374171	70.700071
841.437602	26.826825	70.705076
840.335753	27.177249	70.710081
839.895287	19.314100	70.715086
839.203843	29.979783	70.720090
838.539438	20.671590	70.725095
837.761331	33.020981	70.730100
837.070659	27.719081	70.735105
836.789261	25.778594	70.740110
836.132949	27.683864	70.745114
834.919453	20.716429	70.750119
834.619739	11.966754	70.755124
833.691542	28.304297	70.760129
833.443162	22.025297	70.765134
832.149336	21.994716	70.770138
831.857412	24.907955	70.775143
831.263362	27.571255	70.780148
830.842604	30.632729	70.785153
830.483831	27.432018	70.790158
829.004983	30.012237	70.795162
828.789214	28.655787	70.800167
828.075367	33.846969	70.805172
827.189935	27.428107	70.810177
826.619199	18.254813	70.815182
825.922491	23.419611	70.820186
825.871631	28.983055	70.825191
824.796005	29.297774	70.830196
824.034277	24.357257	70.835201
823.844754	30.157229	70.840206
822.264503	45.758109	70.845210
821.644625	34.537956	70.850215
821.421035	29.002449	70.855220
820.843374	42.702866	70.860225
820.022000	24.477187	70.865230
819.017121	33.705772	70.870234
818.801281	30.012401	70.875239
818.407236	32.159767	70.880244
817.632173	16.618457	70.885249
816.971067	24.693234	70.890254
815.705294	33.006184	70.895258
815.578642	27.504131	70.900263
814.445495	36.094001	70.905268
813.564806	32.501730	70.910273
813.519651	26.958321	70.915278
812.807591	41.906942	70.920282
812.329329	33.433250	70.925287
811.345448	33.151502	70.930292
810.552908	35.512105	70.935297
810.311503	28.607552	70.940302
809.308220	41.699240	70.945306
808.920110	28.723406	70.950311
808.024125	31.079976	70.955316
807.401558	24.035836	70.960321
807.332090	29.413016	70.965326
806.379788	33.181973	70.970330
806.023372	27.743302	70.975335
804.592509	25.910103	70.980340
803.538737	34.101006	70.985345
803.312453	37.629822	70.990350
802.466664	35.577339	70.995354
802.564499	26.920489	71.000359
801.989441	31.860936	71.005364
800.997622	28.909227	71.010369
800.337815	24.029762	71.015374
799.771880	39.847634	71.020378
798.997463	27.195060	71.025383
798.002206	33.187945	71.030388
797.546497	31.354054	71.035393
797.177832	30.933380	71.040398
796.067746	29.500109	71.045402
795.852725	19.685179	71.050407
795.347031	30.652444	71.055412
794.400214	31.173741	71.060417
793.147800	23.269552	71.065422
792.513748	31.261185	71.070426
792.425792	17.764522	71.075431
791.988263	27.905690	71.080436
790.833149	21.946071	71.085441
790.157248	20.546184	71.090446
789.578092	35.478375	71.095450
789.158973	25.145602	71.100455
788.422233	13.504132	71.105460
787.913102	23.549468	71.110465
787.326052	28.241102	71.115470
785.808100	32.782898	71.120474
785.534370	15.684264	71.125479
784.908981	29.116316	71.130484
784.376037	32.067929	71.135489
784.245794	24.647393	71.140494
783.150042	28.808181	71.145498
782.554501	22.948712	71.150503
781.938458	24.708819	71.155508
781.067271	21.851451	71.160513
780.364922	14.938291	71.165518
779.727519	25.630068	71.170522
779.302738	25.156832	71.175527
778.288479	28.076262	71.180532
777.427126	28.864644	71.185537
777.191403	23.313732	71.190542
776.616123	28.754087	71.195546
775.939458	28.620557	71.200551
775.041971	31.116142	71.205556
774.253823	39.485535	71.210561
774.059850	16.345806	71.215566
772.564352	29.047518	71.220570
772.393245	31.731805	71.225575
771.893753	26.027350	71.230580
771.770277	34.286198	71.235585
771.204417	24.254322	71.240590
769.782701	42.441291	71.245594
768.933418	32.427723	71.250599
767.761627	28.591667	71.255604
767.717006	37.072917	71.260609
767.100598	30.852513	71.265614
766.829976	20.210695	71.270618
766.434306	26.284746	71.275623
765.431921	23.698994	71.280628
764.683547	33.585315	71.285633
764.124280	25.949244	71.290638
763.081252	20.805963	71.295642
762.317439	25.724428	71.300647
761.982512	29.858714	71.305652
761.517130	24.356980	71.310657
760.554320	19.856911	71.315662
759.779799	20.046455	71.320666
759.335590	19.491164	71.325671
758.907891	30.941154	71.330676
757.584144	21.804187	71.335681
756.914796	19.367259	71.340686
756.221383	17.613796	71.345690
756.223500	14.510181	71.350695
755.861691	24.849018	71.355700
754.987520	20.599754	71.360705
754.381041	15.462670	71.365710
752.883171	19.750561	71.370714
751.866075	18.632074	71.375719
751.429453	20.194898	71.380724
751.092236	20.436243	71.385729
751.115833	19.333415	71.390734
750.560071	26.213507	71.395738
749.860091	8.550426	71.400743
748.719475	19.421659	71.405748
748.113849	29.075531	71.410753
747.477452	11.328211	71.415758
746.466451	26.947283	71.420762
746.025048	20.974982	71.425767
745.763396	23.951214	71.430772
744.750983	26.922399	71.435777
744.229325	17.947890	71.440782
743.470982	28.312016	71.445786
743.063451	12.980302	71.450791
742.116376	28.021523	71.455796
741.465979	30.298017	71.460801
741.202382	16.495031	71.465806
739.635646	26.650407	71.470810
739.334359	7.041069	71.475815
738.605557	19.567110	71.480820
737.989219	28.248179	71.485825
737.929342	16.678729	71.490830
736.801158	29.837617	71.495834
736.329357	16.922446	71.500839
735.712175	18.261718	71.505844
734.570834	19.309146	71.510849
734.235903	19.851313	71.515854
733.247216	26.483382	71.520858
732.868595	21.675860	71.525863
731.925270	17.573228	71.530868
730.901795	27.594810	71.535873
730.816525	12.561859	71.540878
730.289716	18.875974	71.545882
729.930000	22.446533	71.550887
729.400994	28.395167	71.555892
728.243942	26.188852	71.560897
728.017765	17.408566	71.565902
726.693260	20.986083	71.570906
725.861959	23.617795	71.575911
725.278064	23.937840	71.580916
724.748349	16.185122	71.585921
724.986089	18.745971	71.590926
723.509654	23.123501	71.595930
722.975322	17.441955	71.600935
722.758123	16.044746	71.605940
721.668704	27.402981	71.610945
721.004060	23.043103	71.615950
720.514688	22.034563	71.620954
719.737344	19.449269	71.625959
718.586205	18.278025	71.630964
717.883433	24.837770	71.635969
717.713506	20.905303	71.640974
717.299793	21.228215	71.645978
716.693401	14.985740	71.650983
715.721658	20.809332	71.655988
715.188938	22.600340	71.660993
714.319378	11.766911	71.665998
713.369682	19.982264	71.671002
713.005868	19.961357	71.676007
712.512024	18.371664	71.681012
711.567051	21.917144	71.686017
710.784777	20.712403	71.691022
710.290693	21.965853	71.696026
710.183548	6.796053	71.701031
709.541023	20.814277	71.706036
708.270171	26.013749	71.711041
707.723714	20.294715	71.716046
707.113971	21.662771	71.721050
706.352014	18.083178	71.726055
705.585062	22.076530	71.731060
704.747217	17.553435	71.736065
704.765102	18.927209	71.741070
703.780809	24.161477	71.746074
702.975917	17.827614	71.751079
702.574667	22.770362	71.756084
701.975687	18.966135	71.761089
701.256252	13.903820	71.766094
700.213429	20.292217	71.771098
699.990931	22.046448	71.776103
699.259506	19.133744	71.781108
698.843734	21.429656	71.786113
697.795846	21.952890	71.791118
697.062347	24.668382	71.796122
697.189034	26.452166	71.801127
695.812934	18.632381	71.806132
695.085595	25.596568	71.811137
694.956189	20.743065	71.816142
694.067349	20.821528	71.821146
692.964119	23.857652	71.826151
692.482517	22.330666	71.831156
691.668942	11.991356	71.836161
691.049013	17.803089	71.841166
689.988460	19.110473	71.846170
689.707512	23.122633	71.851175
689.408086	25.535633	71.856180
688.806229	29.879577	71.861185
688.492010	26.343808	71.866190
687.399900	26.166071	71.871194
686.911552	18.857762	71.876199
685.638855	16.078556	71.881204
684.660971	20.446105	71.886209
684.418499	20.438996	71.891214
683.786358	28.774100	71.896218
683.499775	17.912505	71.901223
683.623557	15.447076	71.906228
682.120990	15.711572	71.911233
682.187246	15.316276	71.916238
680.870310	17.973292	71.921242
680.078202	9.743581	71.926247
679.221041	11.299265	71.931252
678.273972	20.841937	71.936257
677.616798	17.822805	71.941262
676.849182	14.439657	71.946266
676.660292	9.723358	71.951271
676.250626	13.970468	71.956276
675.432909	27.321197	71.961281
674.794037	24.953552	71.966286
674.101967	24.276904	71.971290
673.896510	24.937227	71.976295
672.680503	17.834674	71.981300
672.207937	15.057370	71.986305
671.356352	19.338583	71.991310
670.644440	26.557350	71.996314
669.566409	26.229153	72.001319
668.957470	31.573967	72.006324
668.690674	25.307387	72.011329
668.561958	7.118163	72.016334
667.834583	14.358309	72.021338
667.209375	18.471019	72.026343
666.300749	26.612043	72.031348
665.413573	23.225859	72.036353
664.698968	14.841892	72.041358
663.901030	20.524289	72.046362
663.832886	17.837121	72.051367
662.960346	21.891451	72.056372
661.649456	20.606907	72.061377
661.615685	17.627275	72.066382
660.995277	19.443294	72.071386
660.636255	17.308622	72.076391
659.620305	17.981319	72.081396
659.061371	17.906340	72.086401
658.728249	15.993037	72.091406
657.308934	18.768864	72.096410
656.713835	21.720934	72.101415
656.382497	18.347162	72.106420
655.570457	22.044948	72.111425
654.848094	20.564193	72.116430
653.966640	33.280139	72.121434
653.265739	19.023288	72.126439
653.444840	16.536434	72.131444
652.138030	27.703816	72.136449
651.312907	22.905914	72.141454
650.791087	25.830548	72.146458
650.165941	16.407372	72.151463
649.934897	21.370326	72.156468
648.898329	25.048679	72.161473
648.308051	19.519558	72.166478
647.735892	16.130523	72.171482
647.155771	14.947226	72.176487
646.040120	22.592970	72.181492
645.360131	23.560662	72.186497
645.145294	17.542845	72.191502
644.959945	14.926380	72.196506
643.516142	19.273526	72.201511
642.957734	19.737757	72.206516
642.329414	27.507739	72.211521
642.048157	18.576976	72.216526
640.833233	20.134455	72.221530
640.455546	21.708410	72.226535
640.011871	22.176448	72.231540
638.897879	27.398278	72.236545
638.431684	15.150843	72.241550
637.752246	28.902161	72.246554
637.154408	20.110118	72.251559
636.105047	22.365019	72.256564
635.286700	27.173935	72.261569
635.166310	11.216242	72.266574
634.405731	32.055911	72.271578
633.961504	28.460433	72.276583
633.305351	25.456919	72.281588
632.318297	31.970498	72.286593
632.430989	16.650583	72.291598
631.145640	23.963830	72.296602
630.489651	15.802341	72.301607
629.916738	21.068886	72.306612
629.204557	36.421221	72.311617
628.763221	26.005304	72.316622
627.635670	22.329425	72.321626
627.320600	19.069756	72.326631
626.301159	24.180343	72.331636
625.180662	16.010833	72.336641
624.964410	18.349093	72.341646
624.534841	28.337624	72.346650
624.295723	20.948642	72.351655
624.166632	19.422299	72.356660
622.754128	19.828598	72.361665
622.421551	18.459235	72.366670
620.798601	27.133480	72.371674
620.362331	25.108882	72.376679
619.883079	19.185215	72.381684
619.392534	25.443113	72.386689
618.532695	24.249178	72.391694
617.551507	24.503216	72.396698
617.432861	17.020938	72.401703
617.191328	17.008955	72.406708
615.870605	20.209051	72.411713
615.476367	14.919943	72.416718
614.606041	30.885634	72.421722
613.786165	25.885070	72.426727
613.272997	25.780737	72.431732
612.418026	23.433334	72.436737
612.417989	16.198660	72.441742
611.298583	21.342518	72.446746
610.731212	23.265214	72.451751
610.205986	13.100779	72.456756
609.154519	18.864566	72.461761
608.483150	14.452184	72.466766
607.438420	18.656949	72.471770
607.441661	6.454610	72.476775
607.180776	23.466466	72.481780
606.254226	27.335461	72.486785
605.521386	17.484773	72.491790
604.701722	23.339372	72.496794
604.214635	18.279506	72.501799
603.085605	18.391524	72.506804
602.438727	21.284046	72.511809
602.321228	15.783717	72.516814
601.446163	34.128092	72.521818
600.567783	18.065626	72.526823
600.112131	27.022306	72.531828
599.021323	25.964506	72.536833
599.068396	16.366482	72.541838
598.327835	19.505725	72.546842
597.379004	17.789834	72.551847
596.880626	29.880259	72.556852
596.074679	27.354752	72.561857
595.370953	10.449238	72.566862
594.301201	26.840907	72.571866
593.978351	18.236884	72.576871
593.733198	16.378963	72.581876
592.926350	22.641510	72.586881
592.175110	21.064454	72.591886
591.658339	22.848215	72.596890
591.366729	19.909651	72.601895
590.547977	13.423508	72.606900
589.257596	20.341779	72.611905
589.037673	13.542654	72.616910
587.939930	25.594501	72.621914
587.146048	12.265504	72.626919
586.546612	21.027474	72.631924
585.901677	21.098666	72.636929
586.096106	8.807534	72.641934
585.233670	15.570918	72.646938
584.089533	15.399936	72.651943
583.678102	20.284396	72.656948
583.269597	31.827526	72.661953
582.338737	14.135062	72.666958
581.333276	21.995079	72.671962
581.107068	22.275534	72.676967
580.906685	19.160024	72.681972
579.542233	20.154751	72.686977
579.060135	10.141147	72.691982
578.258553	25.810475	72.696986
577.588105	17.774303	72.701991
576.998494	15.411457	72.706996
576.107330	27.591248	72.712001
575.844550	19.222076	72.717006
574.780788	21.843552	72.722010
574.197844	22.953494	72.727015
573.643871	18.367890	72.732020
573.069748	17.208885	72.737025
572.589738	11.460387	72.742030
571.597438	21.667848	72.747034
571.258161	20.786813	72.752039
570.657256	15.864928	72.757044
569.220948	28.552574	72.762049
569.048014	17.143076	72.767054
568.383164	16.712845	72.772058
567.778899	21.829861	72.777063
566.903202	16.828749	72.782068
565.947973	18.985110	72.787073
565.648605	19.261450	72.792078
565.260881	17.881956	72.797082
564.756169	21.265903	72.802087
564.092945	27.029368	72.807092
563.294066	22.720882	72.812097
562.626695	11.368066	72.817102
561.444852	18.108220	72.822106
560.735056	23.000785	72.827111
560.199318	15.512414	72.832116
559.800209	22.782298	72.837121
559.907112	12.454119	72.842126
558.747628	26.010684	72.847130
558.069537	16.151295	72.852135
556.854901	18.429398	72.857140
556.084530	31.361047	72.862145
555.726470	18.342667	72.867150
555.149362	25.519486	72.872154
555.079219	25.948540	72.877159
554.021599	29.370099	72.882164
553.205407	19.354521	72.887169
552.817753	17.922981	72.892174
551.540565	20.187397	72.897178
551.157122	25.936261	72.902183
550.430559	24.284328	72.907188
549.959053	26.718443	72.912193
549.699162	26.370363	72.917198
548.421355	28.385734	72.922202
547.958014	29.547590	72.927207
547.457648	22.748986	72.932212
546.082868	27.589791	72.937217
545.640323	15.734413	72.942222
544.950744	30.774086	72.947226
544.885645	27.264887	72.952231
544.551764	23.238713	72.957236
543.281693	25.926179	72.962241
542.497209	18.474280	72.967246
542.306784	20.072033	72.972250
541.018096	20.201626	72.977255
540.483792	14.357710	72.982260
539.953306	26.137875	72.987265
539.766283	18.890415	72.992270
538.662699	20.691968	72.997274
538.170828	15.858375	73.002279
537.725190	18.583245	73.007284
536.618315	14.309639	73.012289
536.187866	11.274935	73.017294
535.825365	14.923223	73.022298
534.658050	11.094463	73.027303
533.932659	18.890959	73.032308
532.985246	18.184066	73.037313
533.057512	12.265608	73.042318
532.112426	21.591974	73.047322
531.138345	24.358447	73.052327
530.861504	15.258281	73.057332
530.019777	17.049663	73.062337
530.085109	13.011939	73.067342
529.001540	22.794005	73.072346
528.199802	26.832369	73.077351
527.038639	22.406572	73.082356
526.289753	10.434432	73.087361
525.839050	13.503867	73.092366
525.240375	12.903843	73.097370
525.005962	24.528042	73.102375
524.644235	14.731807	73.107380
523.550466	14.168074	73.112385
522.966106	15.298751	73.117390
522.299521	10.455150	73.122394
521.248137	15.908311	73.127399
520.621357	8.656797	73.132404
520.034169	19.017346	73.137409
520.039841	17.917375	73.142414
518.920205	24.579833	73.147418
517.928718	20.609536	73.152423
517.772152	12.835286	73.157428
516.891639	18.092504	73.162433
516.202299	15.750291	73.167438
515.134744	18.681462	73.172442
514.717768	10.117685	73.177447
514.638032	17.724605	73.182452
513.389516	20.206811	73.187457
512.940648	16.865978	73.192462
512.206913	17.776038	73.197466
511.447290	29.589556	73.202471
510.946526	11.287756	73.207476
509.953849	21.526832	73.212481
509.766715	14.512773	73.217486
509.246967	20.057859	73.222490
508.530845	16.480495	73.227495
507.831791	15.374521	73.232500
507.068676	17.738407	73.237505
506.404423	5.787488	73.242510
505.554454	19.069264	73.247514
504.707362	36.619187	73.252519
504.376742	0.712912	73.257524
503.864311	27.222895	73.262529
503.048786	11.740226	73.267534
502.048775	28.253267	73.272538
501.693898	11.869358	73.277543
501.211606	19.822666	73.282548
500.214895	17.810106	73.287553
499.654271	12.687871	73.292558
499.265543	19.278050	73.297562
498.514029	15.222229	73.302567
497.969156	17.032559	73.307572
496.876494	20.049734	73.312577
496.392130	12.696695	73.317582
495.502882	10.468333	73.322586
494.729142	15.490940	73.327591
494.532339	9.615349	73.332596
493.786019	26.051706	73.337601
493.261030	16.235758	73.342606
491.937910	15.073098	73.347610
491.685573	16.996090	73.352615
491.337040	11.977258	73.357620
490.619894	24.875203	73.362625
489.678031	13.764829	73.367630
488.983367	17.240546	73.372634
488.598593	28.969121	73.377639
488.289354	23.532462	73.382644
486.950063	29.706407	73.387649
486.693879	19.004010	73.392654
485.965188	22.341654	73.397658
485.331964	17.718240	73.402663
484.579916	12.128215	73.407668
483.514489	15.913722	73.412673
483.313637	13.734959	73.417678
482.514931	24.676388	73.422682
481.658160	18.940627	73.427687
481.103193	12.753109	73.432692
480.655401	19.031018	73.437697
480.355652	15.250142	73.442702
479.238106	20.482060	73.447706
478.579540	19.830091	73.452711
477.680593	18.932581	73.457716
476.504368	15.835360	73.462721
476.248719	14.203041	73.467726
475.640023	19.276627	73.472730
475.425453	14.506099	73.477735
475.188431	19.129408	73.482740
473.932669	23.300039	73.487745
473.690760	24.251598	73.492750
473.007637	21.447961	73.497754
471.708369	25.081504	73.502759
471.179145	24.278051	73.507764
470.184618	16.835992	73.512769
470.411918	9.899410	73.517774
469.113314	16.259253	73.522778
468.342119	26.276989	73.527783
468.133814	16.957769	73.532788
467.766923	22.610967	73.537793
466.570574	14.433128	73.542798
465.731519	18.947359	73.547802
465.306428	16.760171	73.552807
465.001212	16.392515	73.557812
463.751380	27.729081	73.562817
463.185354	16.251351	73.567822
462.897086	22.221589	73.572826
462.564127	22.038116	73.577831
461.802274	15.494076	73.582836
460.421549	28.218643	73.587841
460.139032	23.022147	73.592846
459.139125	22.626405	73.597850
458.146062	21.720244	73.602855
458.134320	22.379681	73.607860
457.495292	30.447852	73.612865
457.354339	20.056668	73.617870
456.311658	24.177590	73.622874
455.461578	28.258367	73.627879
454.951323	12.353367	73.632884
454.032230	20.064052	73.637889
453.423861	12.484790	73.642894
452.991825	17.188053	73.647898
452.286339	20.115176	73.652903
451.340997	9.765431	73.657908
450.621614	22.682658	73.662913
450.287256	11.123874	73.667918
449.837975	19.813057	73.672922
449.031402	25.742879	73.677927
448.324169	22.731790	73.682932
447.462080	29.082022	73.687937
446.771955	17.397000	73.692942
445.406469	20.807729	73.697946
444.988331	20.495911	73.702951
444.907627	21.010225	73.707956
444.414937	26.563627	73.712961
443.799772	19.499507	73.717966
442.938408	23.564739	73.722970
442.318191	21.705095	73.727975
442.257512	26.347617	73.732980
440.570894	28.939083	73.737985
440.291294	25.541334	73.742990
439.801391	21.973677	73.747994
438.712443	26.242320	73.752999
438.044301	31.785834	73.758004
437.661466	33.411098	73.763009
437.172428	31.008609	73.768014
436.388789	26.924810	73.773018
435.768166	19.571418	73.778023
435.196745	15.220433	73.783028
434.187871	20.078681	73.788033
433.582370	11.984909	73.793038
432.946412	14.347478	73.798042
432.520890	10.512538	73.803047
431.950225	11.191646	73.808052
430.591278	16.003175	73.813057
430.121470	10.352432	73.818062
429.681348	24.959724	73.823066
429.117256	13.235709	73.828071
428.470211	17.659436	73.833076
427.556872	18.159767	73.838081
427.070691	13.946583	73.843086
426.744892	20.282327	73.848090
425.342153	13.985489	73.853095
424.924581	14.141915	73.858100
424.366608	14.103104	73.863105
424.170363	5.080007	73.868110
423.322260	16.322609	73.873114
422.268097	16.091638	73.878119
422.142167	12.535376	73.883124
420.625783	23.427174	73.888129
420.083260	17.236112	73.893134
419.366380	18.000018	73.898138
419.024663	18.943831	73.903143
418.850035	20.255238	73.908148
417.788851	13.486112	73.913153
417.375248	13.818516	73.918158
416.888617	22.652418	73.923162
415.890069	19.460689	73.928167
415.313493	4.589668	73.933172
414.111895	23.545873	73.938177
414.083088	13.146294	73.943182
413.182037	13.638365	73.948186
412.394011	18.877724	73.953191
412.241559	14.909395	73.958196
411.380548	16.287594	73.963201
410.377516	12.568332	73.968206
409.825022	12.935483	73.973210
409.261176	18.199043	73.978215
408.590568	14.165052	73.983220
407.565992	32.046023	73.988225
407.452670	6.947724	73.993230
406.890231	18.707756	73.998234
405.842696	18.477312	74.003239
404.847319	19.222523	74.008244
404.341700	29.820819	74.013249
404.196938	15.445505	74.018254
403.373515	17.789069	74.023258
402.212508	18.477099	74.028263
402.147407	17.541363	74.033268
401.392265	21.047238	74.038273
400.922609	15.323940	74.043278
400.024023	19.601684	74.048282
398.947335	9.479464	74.053287
398.827413	22.696972	74.058292
398.072502	14.806781	74.063297
397.403767	8.022440	74.068302
396.436207	6.093585	74.073306
396.009525	22.652473	74.078311
395.247378	10.985261	74.083316
394.350872	17.090265	74.088321
394.031243	16.658686	74.093326
393.325360	12.046880	74.098330
392.967515	25.223459	74.103335
392.269719	12.060583	74.108340
391.272699	27.753199	74.113345
391.130741	17.765867	74.118350
389.747064	10.231327	74.123354
388.725898	14.549106	74.128359
388.691141	20.557793	74.133364
387.988007	20.438048	74.138369
387.587430	20.862994	74.143374
387.024220	9.309158	74.148378
385.996546	14.906815	74.153383
385.830546	15.516719	74.158388
384.398142	19.143135	74.163393
383.793827	10.831584	74.168398
383.257839	14.655759	74.173402
382.834342	7.994760	74.178407
382.965363	13.830379	74.183412
381.665593	19.559702	74.188417
380.977978	13.207280	74.193422
380.219950	23.730685	74.198426
379.132869	16.066889	74.203431
378.794561	3.390760	74.208436
378.050430	21.173421	74.213441
377.660622	13.939380	74.218446
376.642632	19.738915	74.223450
375.825853	19.657782	74.228455
375.710158	11.736700	74.233460
375.229563	11.654032	74.238465
374.418420	12.888686	74.243470
373.628318	16.699744	74.248474
373.112742	14.265233	74.253479
372.117581	6.443303	74.258484
371.274209	19.631020	74.263489
371.199821	5.722299	74.268494
370.743810	12.706386	74.273498
369.434353	17.300336	74.278503
368.853068	19.717282	74.283508
368.517269	11.892774	74.288513
367.834180	17.241571	74.293518
366.714080	14.242690	74.298522
366.081036	17.595082	74.303527
366.043390	4.614014	74.308532
364.728638	17.301292	74.313537
363.850198	25.871228	74.318542
363.560393	6.197114	74.323546
362.814913	17.541642	74.328551
362.897756	7.766066	74.333556
361.606591	16.747102	74.338561
361.250130	21.802590	74.343566
360.512438	21.366679	74.348570
359.308538	19.951716	74.353575
358.495526	6.944407	74.358580
358.063494	21.947779	74.363585
357.944474	17.859015	74.368590
357.333809	15.662000	74.373594
356.482130	19.433993	74.378599
355.925580	20.134522	74.383604
355.249558	25.945798	74.388609
354.176409	17.168102	74.393614
353.098138	14.933649	74.398618
352.725352	17.695820	74.403623
352.796723	12.993276	74.408628
352.025404	16.832884	74.413633
351.208710	19.314156	74.418638
350.562406	12.117845	74.423642
349.941788	13.981275	74.428647
348.944512	19.470028	74.433652
348.163204	24.948020	74.438657
348.012280	-7.054079	74.443662
347.372867	28.226154	74.448666
346.309133	13.891656	74.453671
345.797468	11.842862	74.458676
345.155150	15.868482	74.463681
344.575330	14.997431	74.468686
343.514911	10.434260	74.473690
342.647304	24.944109	74.478695
342.491489	17.584480	74.483700
341.914726	13.330562	74.488705
341.335064	11.011923	74.493710
340.426143	25.408516	74.498714
339.553984	29.625303	74.503719
339.516265	19.228726	74.508724
338.485545	16.469489	74.513729
337.679786	17.268082	74.518734
337.197901	16.889176	74.523738
336.758254	23.854896	74.528743
336.062657	15.193650	74.533748
335.042647	29.456573	74.538753
334.699006	15.194966	74.543758
334.145600	16.191449	74.548762
333.172397	19.825130	74.553767
332.647224	3.883142	74.558772
331.863267	22.129447	74.563777
331.389672	21.520575	74.568782
330.556102	12.867130	74.573786
329.907143	19.686444	74.578791
329.746175	25.078190	74.583796
328.949431	13.528477	74.588801
327.694118	31.413123	74.593806
327.126498	4.794620	74.598810
326.642691	29.524478	74.603815
326.492085	6.922023	74.608820
324.966255	31.318089	74.613825
324.620712	7.680739	74.618830
324.237948	14.613737	74.623834
323.477275	17.333657	74.628839
322.791808	14.338063	74.633844
322.062035	19.446743	74.638849
321.721834	11.094696	74.643854
320.363987	20.870083	74.648858
319.695699	15.236807	74.653863
319.510983	17.275186	74.658868
318.988073	17.664449	74.663873
318.210165	12.110143	74.668878
317.534666	13.730029	74.673882
316.866892	6.109823	74.678887
315.755095	28.080909	74.683892
314.833299	31.504567	74.688897
314.781350	19.315784	74.693902
314.096845	22.310558	74.698906
313.580770	12.376562	74.703911
312.930848	10.942712	74.708916
312.103878	26.898387	74.713921
311.872466	14.851746	74.718926
310.679264	18.804334	74.723930
310.080307	13.956329	74.728935
309.633224	16.337706	74.733940
308.905340	22.382748	74.738945
308.289119	9.273138	74.743950
307.233867	12.081010	74.748954
306.466742	21.035318	74.753959
306.548098	7.316238	74.758964
305.306109	17.629798	74.763969
304.551799	8.413407	74.768974
304.021291	17.946555	74.773978
303.739513	24.439287	74.778983
303.529549	5.739588	74.783988
302.160914	10.008705	74.788993
301.749758	7.182275	74.793998
300.644461	7.197613	74.799002
299.644325	11.433228	74.804007
299.812167	6.847769	74.809012
298.814591	13.361548	74.814017
298.718616	16.246753	74.819022
297.724395	14.000506	74.824026
296.696721	12.040275	74.829031
296.589125	9.171771	74.834036
295.317218	14.543473	74.839041
294.729932	10.560891	74.844046
294.592325	11.360229	74.849050
293.848819	11.690046	74.854055
293.144539	10.383131	74.859060
291.928328	21.175110	74.864065
291.422338	18.226608	74.869070
290.990267	18.860004	74.874074
290.540230	20.896522	74.879079
289.732162	7.194637	74.884084
288.975563	22.484695	74.889089
288.521888	17.749150	74.894094
287.662096	8.663113	74.899098
286.789797	17.307775	74.904103
286.345474	10.708463	74.909108
285.629225	15.300936	74.914113
285.361473	11.666373	74.919118
284.176503	10.887061	74.924122
283.829682	16.403039	74.929127
283.476841	6.454077	74.934132
281.865179	14.108050	74.939137
281.357039	13.246089	74.944142
280.756151	13.985238	74.949146
280.708133	24.141616	74.954151
280.538886	10.200721	74.959156
279.010511	7.284306	74.964161
278.589316	21.007112	74.969166
278.003013	15.649348	74.974170
276.580150	17.653283	74.979175
276.245931	2.876146	74.984180
275.566341	13.480096	74.989185
275.403484	10.767049	74.994190
274.531359	16.809858	74.999194
273.613109	15.297371	75.004199
273.310404	15.482819	75.009204
272.615050	11.881724	75.014209
271.888171	19.170760	75.019214
270.800881	25.474939	75.024218
270.237622	24.594958	75.029223
270.063335	9.705596	75.034228
269.565585	16.527624	75.039233
269.010822	17.535376	75.044238
268.188278	6.298874	75.049242
266.544257	20.238672	75.054247
266.194733	12.709671	75.059252
265.349708	20.810705	75.064257
265.568292	11.806660	75.069262
265.108839	22.094845	75.074266
263.939246	21.650542	75.079271
263.425787	20.346332	75.084276
262.843185	23.006348	75.089281
261.547451	8.425051	75.094286
260.674292	21.090865	75.099290
260.342217	10.504695	75.104295
259.895745	2.380908	75.109300
259.531535	22.047296	75.114305
259.162641	24.228571	75.119310
258.236138	14.484586	75.124314
257.253259	17.645200	75.129319
256.355180	16.482721	75.134324
255.397327	17.393889	75.139329
254.827581	15.379603	75.144334
254.706893	11.502417	75.149338
254.075924	10.063986	75.154343
253.916026	12.743350	75.159348
252.943336	17.722043	75.164353
252.355575	12.290408	75.169358
251.342703	10.562791	75.174362
250.331519	24.728135	75.179367
250.633611	8.390968	75.184372
249.247715	11.374565	75.189377
248.448074	7.416386	75.194382
247.822267	15.409941	75.199386
247.340055	11.107864	75.204391
247.332329	9.396631	75.209396
246.162792	10.335238	75.214401
245.781062	1.292861	75.219406
244.921199	12.406494	75.224410
243.534765	12.608590	75.229415
243.321037	5.912612	75.234420
242.802767	20.623818	75.239425
242.364538	14.851399	75.244430
241.193887	7.711906	75.249434
240.177351	10.437944	75.254439
240.096995	6.928049	75.259444
239.617867	13.974180	75.264449
239.087961	11.923587	75.269454
238.238028	14.203622	75.274458
237.284643	14.689908	75.279463
237.371303	17.457695	75.284468
236.194728	18.132515	75.289473
235.156573	14.343241	75.294478
234.760774	18.063097	75.299482
234.112997	11.512000	75.304487
233.964378	10.655812	75.309492
232.751971	16.506887	75.314497
232.162330	17.747275	75.319502
231.777704	16.841981	75.324506
230.757409	16.771264	75.329511
230.382123	12.781710	75.334516
229.552712	13.547840	75.339521
229.284622	5.682612	75.344526
228.212978	12.162492	75.349530
227.490558	9.377813	75.354535
227.265503	18.655707	75.359540
225.722440	16.810781	75.364545
224.961455	13.489808	75.369550
224.758242	13.028655	75.374554
224.004525	12.223200	75.379559
223.965073	2.053995	75.384564
222.815891	3.188053	75.389569
222.243799	14.774606	75.394574
221.635587	17.187991	75.399578
220.822991	15.909403	75.404583
220.961199	4.461421	75.409588
219.705275	18.670513	75.414593
219.082374	-2.111012	75.419598
218.324551	5.810553	75.424602
217.000680	9.954313	75.429607
216.311818	16.630206	75.434612
216.109027	13.094100	75.439617
216.025064	10.155606	75.444622
215.827385	3.789793	75.449626
214.571784	11.439077	75.454631
214.295357	8.881329	75.459636
212.817559	12.830446	75.464641
212.281178	9.696010	75.469646
211.626970	6.913076	75.474650
211.399881	11.940065	75.479655
210.771927	-1.125051	75.484660
209.449372	15.884136	75.489665
209.138915	12.065591	75.494670
208.758937	12.821576	75.499674
207.979134	18.501200	75.504679
207.298800	1.268894	75.509684
206.686916	15.495156	75.514689
205.430086	11.622493	75.519694
205.388645	11.849871	75.524698
204.604516	14.283420	75.529703
204.073340	9.457757	75.534708
202.780153	17.704366	75.539713
202.252692	8.489696	75.544718
201.830878	8.769831	75.549722
200.930094	17.195142	75.554727
200.168186	11.805478	75.559732
199.033562	18.229184	75.564737
199.140844	17.972408	75.569742
198.547895	13.394700	75.574746
198.576093	13.778124	75.579751
197.196591	15.275324	75.584756
196.691394	19.050471	75.589761
196.328758	14.472313	75.594766
195.157441	13.881670	75.599770
194.321638	17.296386	75.604775
193.824493	19.947522	75.609780
193.609294	10.689379	75.614785
192.772693	-0.642607	75.619790
192.190732	21.177795	75.624794
191.297309	12.406226	75.629799
190.221704	6.926239	75.634804
189.477375	9.396022	75.639809
189.188459	14.782934	75.644814
189.126990	6.049034	75.649818
188.060153	24.168579	75.654823
187.601596	16.302182	75.659828
186.753571	13.737802	75.664833
185.837634	7.191631	75.669838
184.821025	10.676173	75.674842
184.159809	2.747483	75.679847
184.017308	2.536838	75.684852
183.574776	19.555536	75.689857
182.986017	14.879399	75.694862
181.853160	26.221074	75.699866
181.183869	29.322260	75.704871
181.159389	13.689980	75.709876
179.796542	16.028157	75.714881
178.905636	19.541544	75.719886
178.605928	6.917659	75.724890
178.245011	4.725028	75.729895
177.654759	15.861923	75.734900
176.686916	21.719761	75.739905
175.945404	10.210197	75.744910
175.654433	19.984274	75.749914
174.257002	18.299079	75.754919
174.394201	11.993411	75.759924
173.168413	18.065830	75.764929
172.896416	12.613835	75.769934
171.805158	10.195468	75.774938
171.209408	21.106176	75.779943
170.980829	13.753444	75.784948
170.596579	18.691960	75.789953
169.868565	10.122676	75.794958
168.922747	-0.105427	75.799962
168.072650	17.850256	75.804967
167.174806	8.658383	75.809972
165.930623	14.451478	75.814977
165.979815	11.267842	75.819982
165.733962	9.219284	75.824986
165.121715	15.685864	75.829991
164.543647	12.133909	75.834996
163.205808	16.150621	75.840001
162.713695	10.125055	75.845006
162.399483	2.338154	75.850010
161.108157	14.525062	75.855015
160.777853	16.384824	75.860020
160.194943	15.285665	75.865025
160.063209	14.768969	75.870030
159.233317	5.881641	75.875034
158.228369	23.945596	75.880039
157.839006	9.666108	75.885044
156.572565	19.836978	75.890049
156.029403	18.728329	75.895054
155.848055	9.866896	75.900058
155.162515	11.994597	75.905063
154.276877	16.377581	75.910068
153.455348	2.244275	75.915073
153.219118	15.130232	75.920078
152.412451	4.282317	75.925082
151.203331	13.660344	75.930087
150.970494	4.215801	75.935092
150.304376	8.888616	75.940097
149.618629	18.741407	75.945102
148.886084	17.216704	75.950106
148.115377	2.282134	75.955111
147.698109	16.817974	75.960116
147.151859	11.846504	75.965121
146.538138	8.393274	75.970126
145.681286	12.237113	75.975130
145.048296	4.830608	75.980135
144.173260	3.079484	75.985140
143.116374	17.722040	75.990145
142.889965	10.842028	75.995150
142.627117	14.958565	76.000154
141.732805	24.016763	76.005159
141.504749	1.212271	76.010164
140.297261	5.813722	76.015169
140.036466	17.880476	76.020174
138.960188	0.550497	76.025178
138.126245	20.110434	76.030183
137.810991	4.166588	76.035188
136.972786	6.862653	76.040193
136.758981	15.288821	76.045198
135.790511	13.956273	76.050202
135.002398	14.458820	76.055207
134.414793	10.823244	76.060212
133.688615	23.112434	76.065217
133.082242	11.079896	76.070222
132.514578	17.769596	76.075226
131.923065	15.159604	76.080231
131.529813	4.436578	76.085236
130.697315	9.597949	76.090241
129.844695	3.500575	76.095246
129.135357	2.593463	76.100250
128.160634	12.049233	76.105255
127.737266	3.992756	76.110260
127.250147	9.026519	76.115265
126.783446	5.229750	76.120270
125.595185	4.235012	76.125274
125.012338	16.786755	76.130279
124.632588	10.197687	76.135284
124.238813	11.353254	76.140289
123.663687	14.671234	76.145294
122.933338	13.721744	76.150298
121.949519	17.380845	76.155303
120.982830	7.376850	76.160308
120.535111	11.691591	76.165313
119.771454	9.662532	76.170318
119.544671	16.919161	76.175322
118.107784	21.893079	76.180327
117.484868	16.616891	76.185332
116.801722	8.053089	76.190337
116.592565	10.713505	76.195342
116.596041	5.550314	76.200346
115.232159	20.297025	76.205351
114.926811	7.849086	76.210356
114.240468	10.287567	76.215361
113.116760	11.118010	76.220366
112.387706	11.980132	76.225370
111.650652	18.830880	76.230375
111.518372	13.075935	76.235380
110.773772	15.403866	76.240385
109.864373	10.811995	76.245390
109.428552	6.980345	76.250394
108.894510	19.363469	76.255399
108.172718	5.573803	76.260404
107.117860	15.125933	76.265409
106.835606	9.462710	76.270414
106.318734	10.579565	76.275418
105.008386	16.815299	76.280423
104.557568	9.947426	76.285428
103.792826	20.752633	76.290433
103.433861	13.461703	76.295438
103.088064	3.409170	76.300442
101.848987	22.029257	76.305447
101.350998	6.843070	76.310452
100.837707	16.073890	76.315457
100.078722	8.367387	76.320462
99.491020	3.888217	76.325466
98.861101	19.180172	76.330471
98.473185	6.664986	76.335476
97.509559	13.156073	76.340481
96.646965	10.223488	76.345486
96.528300	7.189617	76.350490
94.903797	15.665714	76.355495
94.717423	2.274772	76.360500
93.915173	14.751123	76.365505
93.382874	11.083086	76.370510
93.470130	11.572201	76.375514
92.469266	10.700551	76.380519
91.903454	7.482535	76.385524
90.881101	10.950683	76.390529
89.527833	5.106619	76.395534
89.162324	12.700741	76.400538
88.739303	17.817326	76.405543
88.208581	0.742559	76.410548
88.099383	0.564453	76.415553
87.081247	13.647633	76.420558
86.556062	10.290682	76.425562
85.670737	6.308383	76.430567
84.908272	1.554330	76.435572
83.996368	4.713146	76.440577
83.406942	9.096219	76.445582
83.338750	10.628776	76.450586
82.140969	11.154096	76.455591
81.530624	3.051760	76.460596
80.993871	14.801416	76.465601
80.314884	12.501839	76.470606
79.311981	5.051851	76.475610
78.878452	5.267647	76.480615
78.483194	7.650255	76.485620
77.775682	6.854824	76.490625
76.543753	3.957495	76.495630
76.317285	4.709517	76.500634
75.587351	17.035578	76.505639
75.718316	7.749061	76.510644
74.193875	11.081256	76.515649
73.463458	8.200137	76.520654
72.888957	7.225809	76.525658
72.337008	7.682829	76.530663
71.598039	6.726846	76.535668
70.923175	6.847098	76.540673
70.265925	1.153807	76.545678
69.854782	9.231419	76.550682
69.041503	19.006796	76.555687
68.540196	9.042143	76.560692
67.500188	17.442387	76.565697
67.396433	6.588058	76.570702
66.317701	9.847600	76.575706
65.650903	2.698812	76.580711
65.467286	8.518341	76.585716
64.374614	13.284434	76.590721
63.542379	6.417481	76.595726
63.256603	11.144769	76.600730
62.887020	6.610324	76.605735
62.029920	5.520228	76.610740
61.100780	5.578539	76.615745
60.637359	10.673184	76.620750
59.980516	3.213746	76.625754
58.570101	13.256233	76.630759
58.113107	18.444468	76.635764
57.987936	3.230380	76.640769
57.489991	14.011964	76.645774
56.394323	11.143373	76.650778
55.253431	12.988927	76.655783
55.341356	3.835426	76.660788
54.839674	11.701989	76.665793
53.926195	20.020563	76.670798
53.376634	12.070953	76.675802
52.692952	8.512221	76.680807
51.817872	-2.053513	76.685812
50.715093	13.290202	76.690817
50.281674	9.801937	76.695822
50.120293	4.053221	76.700826
49.428193	15.729891	76.705831
48.875079	4.603478	76.710836
48.062609	9.667065	76.715841
47.439892	21.780504	76.720846
46.905283	12.081348	76.725850
45.710283	22.400133	76.730855
45.516150	12.285575	76.735860
44.885197	13.578323	76.740865
43.810024	17.862268	76.745870
43.613072	10.796235	76.750874
42.608734	20.674628	76.755879
41.806102	3.529708	76.760884
40.795517	14.304750	76.765889
40.683033	11.802877	76.770894
40.456267	10.645370	76.775898
39.283394	15.752252	76.780903
38.558587	3.440619	76.785908
37.998597	11.392173	76.790913
37.656806	4.126907	76.795918
36.663016	11.592594	76.800922
35.791185	12.222059	76.805927
35.503278	5.542676	76.810932
35.082509	17.325876	76.815937
33.957761	18.307899	76.820942
33.508276	15.930733	76.825946
32.699836	16.261523	76.830951
32.151418	14.079899	76.835956
30.989978	17.929780	76.840961
30.374898	14.912013	76.845966
30.089498	11.816436	76.850970
29.396410	12.877838	76.855975
29.098193	18.160594	76.860980
28.065697	23.016448	76.865985
27.530130	21.026729	76.870990
26.856065	22.736342	76.875994
26.111106	17.749291	76.880999
25.254972	6.972396	76.886004
24.784299	17.111006	76.891009
24.311724	14.182469	76.896014
23.363795	6.304296	76.901018
22.730322	17.713016	76.906023
22.441603	18.443435	76.911028
21.826813	7.686390	76.916033
20.626775	19.847760	76.921038
20.186073	9.141791	76.926042
19.652126	14.563064	76.931047
18.800333	9.542599	76.936052
18.125328	15.199247	76.941057
17.347099	14.071357	76.946062
17.174952	12.428929	76.951066
15.774137	22.119848	76.956071
15.191209	13.439178	76.961076
14.605395	10.363136	76.966081
14.441744	15.485664	76.971086
14.262159	10.394251	76.976090
12.924515	18.894024	76.981095
12.386067	11.548171	76.986100
11.816621	24.179790	76.991105
10.543507	18.375022	76.996110
10.122030	8.038130	77.001114
9.545605	17.763126	77.006119
9.293645	11.920056	77.011124
8.218775	18.643371	77.016129
7.367636	18.880061	77.021134
6.905579	13.608212	77.026139
6.638277	10.161265	77.031143
5.812964	4.409651	77.036148
5.123243	16.514855	77.041153
4.318986	23.043631	77.046158