Mon Mar 08 18:54:50 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-2.080120	103.178787	0.000000
-2.024515	65.760367	0.005005
-3.103987	63.445843	0.010010
-4.933041	9.134049	0.015014
-8.853968	-5.651184	0.020019
-14.240634	-4.219606	0.025024
-18.949013	6.544440	0.030029
-23.543896	14.904612	0.035034
-27.235282	-2.090115	0.040038
-31.168468	-0.959716	0.045043
-34.648679	-2.692599	0.050048
-38.279267	11.341848	0.055053
-42.313468	1.658524	0.060058
-45.860820	1.524262	0.065062
-49.646346	9.149863	0.070067
-53.138715	-12.662313	0.075072
-57.005336	8.996057	0.080077
-61.127825	-4.629480	0.085082
-64.525035	-15.620657	0.090086
-68.595870	-4.127227	0.095091
-72.362976	10.928769	0.100096
-75.904984	-5.870517	0.105101
-79.910340	-5.982126	0.110106
-83.722523	6.745750	0.115110
-87.060204	-13.840597	0.120115
-91.177606	-3.068209	0.125120
-94.672783	4.369220	0.130125
-98.282951	4.711805	0.135130
-101.848867	-0.536311	0.140134
-106.163674	-11.182356	0.145139
-110.184553	12.413424	0.150144
-113.624046	-3.670495	0.155149
-117.570979	-18.208537	0.160154
-121.153779	15.186898	0.165158
-124.802957	-10.058190	0.170163
-128.698639	1.238670	0.175168
-132.433484	9.275751	0.180173
-136.324324	1.324762	0.185178
-139.797054	4.783421	0.190182
-143.726809	0.974745	0.195187
-147.994513	14.224801	0.200192
-151.118946	-0.931679	0.205197
-155.054006	6.268532	0.210202
-158.785473	5.435304	0.215206
-162.245839	-1.573561	0.220211
-166.407629	8.986855	0.225216
-170.251421	-11.105471	0.230221
-174.473939	15.881275	0.235226
-178.146800	-3.055680	0.240230
-181.865304	9.338866	0.245235
-185.314740	-9.617951	0.250240
-189.003976	20.005377	0.255245
-193.223674	13.010492	0.260250
-196.315925	-5.139193	0.265254
-200.046099	23.276510	0.270259
-203.715483	-4.724719	0.275264
-207.419609	20.074261	0.280269
-211.589046	-0.908998	0.285274
-215.384430	13.047914	0.290278
-218.932495	-0.883452	0.295283
-223.120981	12.461309	0.300288
-226.206845	-9.377608	0.305293
-230.423486	11.461706	0.310298
-233.753441	6.969291	0.315302
-237.966930	3.808410	0.320307
-241.951397	1.684825	0.325312
-245.513016	3.276632	0.330317
-249.374128	8.106216	0.335322
-252.621594	-3.059960	0.340326
-256.444690	19.194106	0.345331
-260.254686	-16.191039	0.350336
-264.043491	19.350421	0.355341
-267.792183	-0.819994	0.360346
-271.887036	10.196657	0.365350
-275.511996	7.383429	0.370355
-279.257475	-13.474968	0.375360
-282.878428	-7.351228	0.380365
-286.808522	5.744242	0.385370
-290.266145	1.008953	0.390374
-294.240078	7.412967	0.395379
-298.182721	9.440960	0.400384
-301.497776	3.391489	0.405389
-305.751111	2.752168	0.410394
-309.434271	0.205311	0.415398
-313.117962	13.311955	0.420403
-316.928272	9.112363	0.425408
-320.497576	-10.009589	0.430413
-324.710688	8.919735	0.435418
-328.229740	0.887650	0.440422
-331.914443	-0.793234	0.445427
-335.908595	-8.312674	0.450432
-339.235393	2.456901	0.455437
-343.260038	21.903352	0.460442
-346.730851	-3.379283	0.465446
-350.203246	-5.316365	0.470451
-354.411548	1.678630	0.475456
-358.233453	13.232127	0.480461
-362.199154	6.673216	0.485466
-365.652191	-5.607921	0.490470
-369.440812	9.858749	0.495475
-373.149531	3.536358	0.500480
-377.088850	-14.157714	0.505485
-381.093355	19.387340	0.510490
-384.554486	1.791949	0.515494
-388.517424	-4.049885	0.520499
-392.621435	11.979649	0.525504
-395.426168	2.196852	0.530509
-399.394286	-8.742091	0.535514
-403.016310	9.019149	0.540518
-407.439112	-12.311160	0.545523
-411.354440	3.745035	0.550528
-414.536138	-9.123358	0.555533
-418.427064	-7.696325	0.560538
-422.155061	2.662781	0.565542
-425.715422	2.572153	0.570547
-429.815157	-11.759597	0.575552
-433.369733	6.612188	0.580557
-437.525149	19.543612	0.585562
-440.868518	3.154723	0.590566
-445.035278	-0.598258	0.595571
-449.076597	-2.228324	0.600576
-452.247733	0.895629	0.605581
-455.759250	6.322526	0.610586
-459.415845	-10.383708	0.615590
-463.516084	4.588837	0.620595
-467.349711	9.483753	0.625600
-470.868026	2.609179	0.630605
-474.757670	4.688915	0.635610
-478.622495	3.573150	0.640614
-482.121982	16.319478	0.645619
-486.533436	5.178682	0.650624
-489.575574	7.397472	0.655629
-493.722703	10.535425	0.660634
-497.405100	7.684407	0.665638
-501.402527	-7.824112	0.670643
-504.958810	6.363086	0.675648
-508.531523	8.926813	0.680653
-512.544891	9.545707	0.685658
-516.103760	-3.654940	0.690662
-520.084258	-6.038869	0.695667
-524.157592	12.665031	0.700672
-527.366959	8.104898	0.705677
-530.972968	7.077185	0.710682
-534.974174	-3.550327	0.715686
-538.826684	8.766783	0.720691
-542.512418	9.281364	0.725696
-546.420915	1.693417	0.730701
-550.427404	15.689257	0.735706
-554.019940	14.787151	0.740710
-557.348826	9.194390	0.745715
-561.398070	11.523670	0.750720
-564.669940	0.467500	0.755725
-568.932644	7.725421	0.760730
-572.563879	3.948625	0.765734
-576.126251	1.045447	0.770739
-580.262055	2.284791	0.775744
-584.110758	15.793462	0.780749
-587.941162	18.851025	0.785754
-591.415149	3.605955	0.790758
-594.995155	8.681315	0.795763
-599.140657	18.216460	0.800768
-602.611258	-2.915499	0.805773
-606.598674	8.064020	0.810778
-610.234874	10.999137	0.815782
-613.916413	3.408165	0.820787
-618.053950	14.022206	0.825792
-621.607975	8.954328	0.830797
-625.467510	6.576481	0.835802
-629.320268	8.762529	0.840806
-633.091325	8.217047	0.845811
-636.519883	2.939930	0.850816
-640.304160	4.435434	0.855821
-644.421839	14.344649	0.860826
-647.601603	3.718557	0.865830
-651.033167	3.591921	0.870835
-655.530503	2.057139	0.875840
-659.142815	8.766635	0.880845
-663.100957	12.257857	0.885850
-666.920667	12.489703	0.890854
-670.612341	8.104593	0.895859
-674.192298	3.061441	0.900864
-677.534921	3.530872	0.905869
-681.928475	10.951810	0.910874
-685.627799	6.615252	0.915878
-688.766327	-2.672314	0.920883
-692.939433	3.286373	0.925888
-696.546140	4.338884	0.930893
-700.792032	13.576441	0.935898
-704.454100	-3.659900	0.940902
-708.463148	4.670980	0.945907
-712.152228	5.514341	0.950912
-715.223482	7.556729	0.955917
-719.306635	1.785133	0.960922
-722.899523	6.222538	0.965926
-726.975458	10.631488	0.970931
-730.543657	1.172958	0.975936
-734.215655	7.612998	0.980941
-738.381427	4.730802	0.985946
-742.053716	-0.242298	0.990950
-745.850161	3.730963	0.995955
-749.590514	10.721231	1.000960
-753.230542	1.277369	1.005965
-757.285043	16.167385	1.010970
-760.751526	5.147337	1.015974
-764.367729	4.004924	1.020979
-768.566717	10.269056	1.025984
-771.614804	15.879368	1.030989
-775.682979	2.374209	1.035994
-779.213162	3.266392	1.040998
-783.177797	3.996217	1.046003
-787.100419	2.235806	1.051008
-790.870949	-5.392684	1.056013
-794.873141	5.239429	1.061018
-798.551856	1.521037	1.066022
-802.443106	5.388122	1.071027
-806.095085	9.051403	1.076032
-809.268133	-1.914543	1.081037
-813.274418	6.048660	1.086042
-816.875915	3.197834	1.091046
-820.956879	16.168429	1.096051
-824.385066	-2.667739	1.101056
-828.088120	-16.965947	1.106061
-832.564689	7.132585	1.111066
-835.692373	-10.600491	1.116070
-839.946712	5.113158	1.121075
-843.832525	1.459479	1.126080
-847.021470	-3.477177	1.131085
-850.785653	2.722321	1.136090
-854.638066	0.165535	1.141094
-858.736710	7.650023	1.146099
-862.787877	5.560228	1.151104
-866.153743	-6.027621	1.156109
-869.897791	10.750875	1.161114
-873.446339	11.786473	1.166118
-876.897063	-1.192766	1.171123
-880.793955	5.144680	1.176128
-884.898275	-1.850016	1.181133
-889.002134	12.593960	1.186138
-892.068704	-4.210585	1.191142
-896.026428	-13.434691	1.196147
-900.134768	10.786427	1.201152
-903.478698	-0.837989	1.206157
-907.556233	-2.210757	1.211162
-911.521992	3.918566	1.216166
-915.348877	0.839018	1.221171
-918.836286	3.774464	1.226176
-922.294256	-1.199495	1.231181
-926.135888	-2.144778	1.236186
-930.016224	-11.267664	1.241190
-933.638291	7.506615	1.246195
-937.661309	11.503788	1.251200
-941.014317	-3.115114	1.256205
-945.089938	2.989254	1.261210
-948.626208	-1.609472	1.266214
-952.483249	4.964549	1.271219
-956.629783	14.341185	1.276224
-960.012399	-9.448584	1.281229
-964.147426	18.187610	1.286234
-967.527069	-1.272628	1.291238
-970.940310	4.740063	1.296243
-975.131013	-0.838845	1.301248
-978.976361	6.304165	1.306253
-983.071106	10.380686	1.311258
-986.241594	-11.060349	1.316262
-990.097660	11.622567	1.321267
-993.597215	-8.931692	1.326272
-997.470202	6.859997	1.331277
-1001.605635	5.326353	1.336282
-1005.694089	2.213095	1.341286
-1008.607522	-26.792086	1.346291
-1013.019019	13.138826	1.351296
-1016.822407	-19.617257	1.356301
-1020.450165	21.315793	1.361306
-1023.897301	-17.722619	1.366310
-1027.554338	2.154850	1.371315
-1031.588252	4.111915	1.376320
-1035.077985	-8.862399	1.381325
-1039.719747	-4.450739	1.386330
-1043.099937	18.974536	1.391334
-1046.453374	-10.165239	1.396339
-1050.275794	-0.360933	1.401344
-1053.605944	1.225014	1.406349
-1058.116619	10.070317	1.411354
-1062.015205	6.832181	1.416358
-1065.051688	3.219645	1.421363
-1069.040818	-7.300023	1.426368
-1073.057336	-6.545644	1.431373
-1076.896456	9.114601	1.436378
-1080.366391	10.653563	1.441382
-1084.094611	5.838183	1.446387
-1088.124092	7.502920	1.451392
-1091.947370	-1.354444	1.456397
-1095.637314	4.488230	1.461402
-1099.242431	-8.544788	1.466406
-1102.705160	-1.164767	1.471411
-1106.967327	-2.443001	1.476416
-1110.086419	-2.082824	1.481421
-1114.381007	-0.076038	1.486426
-1118.174433	6.661522	1.491430
-1121.760031	-9.409992	1.496435
-1125.750048	-3.661190	1.501440
-1129.394531	0.496507	1.506445
-1133.321565	3.616122	1.511450
-1136.799959	-2.748164	1.516454
-1140.723336	-2.380702	1.521459
-1144.256756	-8.964812	1.526464
-1148.089571	-9.261481	1.531469
-1152.221737	6.429983	1.536474
-1155.778954	8.432417	1.541478
-1159.268650	0.693394	1.546483
-1163.316250	-4.185866	1.551488
-1166.731304	-5.544321	1.556493
-1170.664864	3.175744	1.561498
-1174.671241	-5.242204	1.566502
-1178.233303	-2.217172	1.571507
-1182.262750	6.455180	1.576512
-1185.592109	6.122177	1.581517
-1189.517135	8.894661	1.586522
-1193.352229	4.446619	1.591526
-1197.078558	-0.520249	1.596531
-1201.111024	-2.145697	1.601536
-1204.520225	0.146918	1.606541
-1208.300167	18.581012	1.611546
-1211.964545	-5.428158	1.616550
-1215.957727	7.079618	1.621555
-1219.514239	1.065402	1.626560
-1223.265385	0.867744	1.631565
-1227.312072	20.866196	1.636570
-1230.847957	-7.400457	1.641574
-1234.477944	-9.590102	1.646579
-1238.541069	13.996708	1.651584
-1241.974757	-7.017060	1.656589
-1246.272713	0.939902	1.661594
-1249.896486	25.257477	1.666598
-1253.409681	8.550156	1.671603
-1257.621576	6.992939	1.676608
-1260.655782	-3.743837	1.681613
-1264.773723	-3.925307	1.686618
-1268.260125	26.884214	1.691622
-1272.187262	-6.903334	1.696627
-1276.372169	25.720954	1.701632
-1279.704438	-11.307553	1.706637
-1283.852369	21.552075	1.711642
-1287.212860	-7.633455	1.716646
-1290.813906	-2.575785	1.721651
-1294.931023	25.453825	1.726656
-1298.271155	-0.109811	1.731661
-1302.335119	-3.658508	1.736666
-1305.854605	13.297541	1.741670
-1309.828171	-15.111777	1.746675
-1314.224655	24.268460	1.751680
-1317.604508	3.824888	1.756685
-1321.002250	8.197260	1.761690
-1324.514383	11.175101	1.766694
-1328.331929	-8.648067	1.771699
-1332.658747	17.239117	1.776704
-1336.554625	-1.289541	1.781709
-1340.558786	1.169454	1.786714
-1343.863192	7.132135	1.791718
-1347.293297	9.433034	1.796723
-1351.175724	-5.704397	1.801728
-1354.649452	-3.767062	1.806733
-1359.010457	10.975847	1.811738
-1362.493799	-13.459370	1.816742
-1366.400082	13.134771	1.821747
-1370.084583	-7.226818	1.826752
-1373.853999	-5.573259	1.831757
-1377.456631	13.006139	1.836762
-1381.520612	-13.253530	1.841766
-1384.961838	5.061931	1.846771
-1388.868547	-21.235499	1.851776
-1392.565638	11.272993	1.856781
-1396.653833	3.045148	1.861786
-1399.893731	-30.625027	1.866790
-1403.657950	22.788823	1.871795
-1407.969477	12.520054	1.876800
-1411.713791	-7.537015	1.881805
-1415.303572	-16.457990	1.886810
-1419.035482	15.406464	1.891814
-1422.490150	-17.122383	1.896819
-1426.458739	19.398514	1.901824
-1430.150398	-11.638550	1.906829
-1433.877460	26.906203	1.911834
-1437.903186	2.545311	1.916838
-1441.715101	-8.318985	1.921843
-1445.450790	7.434046	1.926848
-1449.008517	6.034202	1.931853
-1452.580471	3.299489	1.936858
-1456.346109	-2.997806	1.941862
-1460.238628	-7.305316	1.946867
-1464.345335	14.727749	1.951872
-1467.752717	-5.023649	1.956877
-1471.996793	1.152730	1.961882
-1475.553575	6.768098	1.966886
-1478.828428	-8.352841	1.971891
-1482.936688	13.336750	1.976896
-1486.656931	-8.177873	1.981901
-1490.520742	-13.289378	1.986906
-1494.114172	3.801744	1.991910
-1497.698862	-5.528315	1.996915
-1502.000407	4.610826	2.006912
-1502.819331	-9.543426	2.016909
-1500.317343	0.054835	2.026906
-1497.394388	-0.394211	2.036902
-1495.402686	-0.591514	2.046899
-1493.865625	-0.319726	2.056896
-1491.802926	1.274652	2.066893
-1489.643609	-6.262714	2.076890
-1487.809634	-11.346553	2.086886
-1485.957625	6.070058	2.096883
-1483.975353	-0.199561	2.106880
-1481.895892	-5.534269	2.116877
-1480.376866	4.106151	2.126874
-1478.295299	-1.898326	2.136870
-1476.482702	-7.120831	2.146867
-1474.325631	-7.204076	2.156864
-1472.498235	-8.044484	2.166861
-1470.751577	-3.094954	2.176858
-1468.774443	-14.564461	2.186854
-1466.814827	-0.659059	2.196851
-1465.242604	-5.756233	2.206848
-1463.442883	-6.964811	2.216845
-1461.307500	-2.986929	2.226842
-1459.289128	-6.267227	2.236838
-1457.252305	-18.020999	2.246835
-1455.888946	5.683488	2.256832
-1453.942093	-2.053503	2.266829
-1451.818231	-15.591099	2.276826
-1449.805997	-3.261903	2.286822
-1447.902104	8.082080	2.296819
-1446.430740	-6.590451	2.306816
-1444.607411	-1.852110	2.316813
-1442.277840	-8.581480	2.326810
-1440.517741	0.950903	2.336806
-1438.487221	6.507083	2.346803
-1436.849018	-0.831555	2.356800
-1435.082057	3.282702	2.366797
-1433.377315	2.095667	2.376794
-1431.215163	2.753709	2.386790
-1429.257703	-5.883325	2.396787
-1427.366807	7.415796	2.406784
-1425.500854	9.960625	2.416781
-1423.800198	4.231896	2.426778
-1421.727335	10.441274	2.436774
-1419.764326	4.558449	2.446771
-1418.004404	3.918348	2.456768
-1416.006639	9.855560	2.466765
-1414.394345	3.349979	2.476762
-1412.415722	-11.433736	2.486758
-1410.540010	2.183597	2.496755
-1408.668317	1.279310	2.506752
-1406.630266	-1.345715	2.516749
-1405.079889	-1.334931	2.526746
-1402.931158	-9.961512	2.536742
-1400.716330	4.043624	2.546739
-1399.157925	0.510185	2.556736
-1397.479089	5.308013	2.566733
-1395.689708	-4.244665	2.576730
-1393.486733	-3.675223	2.586726
-1391.457977	-17.353853	2.596723
-1390.006157	-2.609241	2.606720
-1387.940061	-3.509897	2.616717
-1385.990861	-3.449265	2.626714
-1384.254508	14.124910	2.636710
-1382.110277	4.359127	2.646707
-1380.552445	2.050980	2.656704
-1378.631986	-3.992357	2.666701
-1376.639535	-2.397681	2.676698
-1374.859227	3.470171	2.686694
-1372.828285	-6.978473	2.696691
-1371.104887	12.277683	2.706688
-1368.982325	-6.847209	2.716685
-1366.963133	-2.992733	2.726682
-1365.618083	-2.273307	2.736678
-1363.832138	8.666504	2.746675
-1361.641123	1.482569	2.756672
-1359.558157	-7.237655	2.766669
-1358.062481	-4.884541	2.776666
-1356.088409	-1.679635	2.786662
-1354.130001	-13.589719	2.796659
-1352.197120	4.714024	2.806656
-1350.253034	1.226245	2.816653
-1348.406652	1.162849	2.826650
-1346.640121	-1.863902	2.836646
-1344.735194	-5.454347	2.846643
-1342.635174	-4.326832	2.856640
-1341.138542	-11.620641	2.866637
-1339.304788	-6.931247	2.876634
-1337.306388	-7.306317	2.886630
-1335.350336	-5.468951	2.896627
-1333.186003	-15.225269	2.906624
-1331.531950	-1.903945	2.916621
-1329.760465	-8.423895	2.926618
-1327.832199	-5.642659	2.936614
-1326.009504	-2.134042	2.946611
-1324.099651	-0.545046	2.956608
-1322.308242	7.896184	2.966605
-1320.226103	-2.213271	2.976602
-1318.558871	-2.514797	2.986598
-1316.618541	1.707590	2.996595
-1314.681477	-9.745923	3.006592
-1313.030890	6.774734	3.016589
-1311.096532	0.722907	3.026586
-1309.043012	-4.650134	3.036582
-1307.071208	1.968659	3.046579
-1305.064816	-6.074570	3.056576
-1303.466240	5.539451	3.066573
-1301.616699	-10.406091	3.076570
-1299.709672	10.630108	3.086566
-1298.040794	-1.473596	3.096563
-1295.829741	-5.627701	3.106560
-1293.822280	-8.932954	3.116557
-1292.268368	7.336367	3.126554
-1290.698450	-7.913934	3.136550
-1288.556513	-0.795016	3.146547
-1286.446157	1.935012	3.156544
-1284.709781	-0.275337	3.166541
-1282.522958	-3.842956	3.176538
-1280.737051	-1.957789	3.186534
-1278.973659	4.888582	3.196531
-1277.116137	-1.918245	3.206528
-1275.161404	0.933008	3.216525
-1273.550954	-10.935548	3.226522
-1271.560591	1.266287	3.236518
-1269.667792	-6.518750	3.246515
-1267.864543	4.648888	3.256512
-1265.915469	2.916064	3.266509
-1264.043409	-1.294287	3.276506
-1262.428529	5.890056	3.286502
-1260.248595	-4.888644	3.296499
-1258.125894	6.632072	3.306496
-1256.682013	2.959163	3.316493
-1254.724420	0.751329	3.326490
-1252.845621	3.619490	3.336486
-1250.682799	-2.874613	3.346483
-1249.021135	-1.831594	3.356480
-1247.151595	-1.835462	3.366477
-1245.339746	2.884361	3.376474
-1243.366980	1.075138	3.386470
-1241.736334	-5.485371	3.396467
-1239.554561	5.834870	3.406464
-1237.569834	6.726736	3.416461
-1235.990544	7.525593	3.426458
-1233.888240	3.133168	3.436454
-1231.857750	2.963042	3.446451
-1230.362928	10.177674	3.456448
-1228.420708	9.991676	3.466445
-1226.315735	12.700520	3.476442
-1224.754735	4.924391	3.486438
-1222.771412	1.002567	3.496435
-1220.766507	11.886950	3.506432
-1219.036070	12.773733	3.516429
-1217.115274	7.594095	3.526426
-1215.188011	2.396058	3.536422
-1213.366960	1.185837	3.546419
-1211.572529	3.841755	3.556416
-1209.609509	-5.508068	3.566413
-1207.772951	2.769728	3.576410
-1205.912219	-1.198780	3.586406
-1203.853221	4.815667	3.596403
-1202.195610	-4.085837	3.606400
-1199.805330	12.463414	3.616397
-1198.469242	3.968592	3.626394
-1196.910658	2.817744	3.636390
-1194.470533	1.203771	3.646387
-1192.639841	-6.849153	3.656384
-1191.105143	11.262699	3.666381
-1188.622067	-5.350949	3.676378
-1187.309229	2.088604	3.686374
-1185.269891	5.494788	3.696371
-1183.328242	-1.274907	3.706368
-1181.142807	-1.240844	3.716365
-1179.487470	3.500916	3.726362
-1177.729224	6.950500	3.736358
-1175.861473	-2.099865	3.746355
-1173.982680	5.028114	3.756352
-1171.907334	7.773326	3.766349
-1170.250535	6.835717	3.776346
-1168.415501	2.482949	3.786342
-1166.455623	7.450721	3.796339
-1164.673752	4.601637	3.806336
-1162.745058	2.122202	3.816333
-1160.834857	0.924600	3.826330
-1158.951534	7.623999	3.836326
-1156.835785	-2.984885	3.846323
-1155.173720	3.012586	3.856320
-1153.254388	10.072525	3.866317
-1151.508447	4.725133	3.876314
-1149.519885	8.035269	3.886310
-1147.765807	1.396653	3.896307
-1145.669182	7.875637	3.906304
-1143.706512	6.723336	3.916301
-1142.345716	-4.202109	3.926298
-1140.135552	-2.795202	3.936294
-1138.173558	-1.572792	3.946291
-1136.492368	0.182407	3.956288
-1134.738054	-2.881706	3.966285
-1132.555402	-2.204559	3.976282
-1130.616447	-4.862441	3.986278
-1128.878032	0.458139	3.996275
-1127.080549	-0.872976	4.006272
-1125.183227	10.966550	4.016269
-1123.307157	-0.968102	4.026266
-1121.497144	5.630958	4.036262
-1119.297486	2.816125	4.046259
-1117.896165	8.836390	4.056256
-1115.787725	0.615937	4.066253
-1113.954154	0.916334	4.076250
-1111.849408	8.137693	4.086246
-1110.386245	11.931357	4.096243
-1108.220780	0.323034	4.106240
-1106.096320	-0.253571	4.116237
-1104.733084	1.579350	4.126234
-1102.592302	-2.932793	4.136230
-1100.422704	6.199671	4.146227
-1098.963932	10.759791	4.156224
-1097.015023	2.340671	4.166221
-1095.048343	7.239528	4.176218
-1093.182559	6.704311	4.186214
-1091.390782	6.274084	4.196211
-1089.574412	1.510700	4.206208
-1087.541643	9.997209	4.216205
-1085.854212	4.553437	4.226202
-1083.864393	3.897341	4.236198
-1082.014701	4.850410	4.246195
-1080.024952	-4.134141	4.256192
-1078.407292	2.484668	4.266189
-1076.359972	0.164739	4.276186
-1074.507067	0.075255	4.286182
-1072.606088	-3.370672	4.296179
-1070.436831	3.418853	4.306176
-1068.894017	3.011096	4.316173
-1067.067387	5.129905	4.326170
-1065.532563	3.490340	4.336166
-1063.170830	-0.930800	4.346163
-1061.333168	-0.779428	4.356160
-1059.540102	-0.030430	4.366157
-1057.766431	4.555138	4.376154
-1055.907249	2.683713	4.386150
-1053.415719	-3.161779	4.396147
-1051.842477	1.825300	4.406144
-1050.190360	5.533523	4.416141
-1048.150975	3.753277	4.426138
-1046.349489	9.092259	4.436134
-1044.448446	2.545465	4.446131
-1042.588129	2.911111	4.456128
-1040.762728	0.165677	4.466125
-1038.980221	2.736803	4.476122
-1036.787307	2.600867	4.486118
-1035.044098	-2.226562	4.496115
-1033.342341	4.603030	4.506112
-1031.295407	-2.102865	4.516109
-1029.399742	7.158739	4.526106
-1027.742242	-6.588154	4.536102
-1025.554370	4.870278	4.546099
-1023.712702	4.667374	4.556096
-1022.086379	-1.947567	4.566093
-1020.293344	9.454024	4.576090
-1017.987274	6.567005	4.586086
-1016.286298	1.526880	4.596083
-1014.571931	5.485687	4.606080
-1012.737834	7.249682	4.616077
-1010.637594	11.707281	4.626074
-1008.775551	2.908982	4.636070
-1006.864438	1.474529	4.646067
-1005.024005	5.998940	4.656064
-1003.170196	4.927318	4.666061
-1001.193110	2.402380	4.676058
-999.421279	-1.153883	4.686054
-997.625209	11.020884	4.696051
-995.650441	-6.144434	4.706048
-993.745034	5.027641	4.716045
-991.964599	5.661876	4.726042
-990.203663	-5.570627	4.736038
-988.486561	3.321694	4.746035
-986.119891	-10.028602	4.756032
-984.171495	3.283852	4.766029
-982.941115	3.612913	4.776026
-980.630361	-0.449489	4.786022
-978.884959	13.313837	4.796019
-976.826109	3.315733	4.806016
-975.034596	7.039616	4.816013
-973.354543	10.200304	4.826010
-971.156787	3.254034	4.836006
-969.231238	-2.110898	4.846003
-967.679195	-1.192244	4.856000
-965.530470	8.992060	4.865997
-963.934239	-5.755473	4.875994
-962.093157	-2.473694	4.885990
-960.242118	8.931306	4.895987
-957.998605	-1.145251	4.905984
-956.208835	1.971064	4.915981
-954.234093	7.781339	4.925978
-952.521850	5.275104	4.935974
-950.682360	8.784505	4.945971
-948.785807	11.244316	4.955968
-946.933390	9.885608	4.965965
-944.910592	5.304046	4.975962
-943.331138	4.175290	4.985958
-941.126176	13.940128	4.995955
-939.283189	7.527422	5.005952
-937.520321	5.463078	5.015949
-935.892763	8.430092	5.025946
-933.968402	8.124043	5.035942
-931.769359	8.812969	5.045939
-929.843798	0.686638	5.055936
-927.957871	0.208327	5.065933
-926.197065	5.168669	5.075930
-924.384605	-3.449545	5.085926
-922.831099	18.052507	5.095923
-920.528586	2.541579	5.105920
-918.491323	4.745247	5.115917
-916.749713	15.815702	5.125914
-915.188431	6.162441	5.135910
-913.173800	7.411364	5.145907
-911.267325	6.677164	5.155904
-909.326935	-0.262641	5.165901
-907.537402	11.588008	5.175898
-905.759777	4.918949	5.185894
-903.749948	1.474696	5.195891
-901.670826	1.668113	5.205888
-900.149429	13.689525	5.215885
-898.200790	6.712093	5.225882
-896.059466	3.082623	5.235878
-894.024904	11.199579	5.245875
-892.387071	0.675196	5.255872
-890.736406	1.241838	5.265869
-888.738372	5.051189	5.275866
-887.011354	14.456724	5.285862
-885.137763	1.922657	5.295859
-883.057189	11.364827	5.305856
-881.043592	5.201190	5.315853
-879.395244	-1.477181	5.325850
-877.519827	11.458652	5.335846
-875.614340	4.500768	5.345843
-873.762683	4.711625	5.355840
-871.676347	11.811434	5.365837
-869.945382	3.391007	5.375834
-868.274167	13.539648	5.385830
-866.176481	-9.843841	5.395827
-864.326383	8.805207	5.405824
-862.087100	8.952532	5.415821
-860.809039	5.975795	5.425818
-858.925214	6.595184	5.435814
-856.893681	-2.970586	5.445811
-854.900040	0.989488	5.455808
-852.963915	5.490836	5.465805
-851.163246	11.453761	5.475802
-849.403043	6.759523	5.485798
-847.302198	1.035101	5.495795
-845.642990	5.422833	5.505792
-843.708339	-4.714776	5.515789
-841.624834	4.990631	5.525786
-839.896240	8.112082	5.535782
-838.315223	0.516128	5.545779
-835.956301	5.628820	5.555776
-834.377636	-0.771557	5.565773
-832.664176	-0.202281	5.575770
-830.611613	9.056532	5.585766
-828.668182	0.614803	5.595763
-826.554474	1.559034	5.605760
-824.855030	3.993613	5.615757
-823.026682	-3.292934	5.625754
-821.300701	-0.707866	5.635750
-819.356337	10.407626	5.645747
-817.698777	-0.460901	5.655744
-815.270715	4.252362	5.665741
-813.667062	10.437849	5.675738
-811.598780	7.339572	5.685734
-809.871626	-1.381768	5.695731
-808.056038	8.552802	5.705728
-806.397576	0.205581	5.715725
-804.520291	8.305129	5.725722
-802.226311	10.216832	5.735718
-800.769145	12.728046	5.745715
-798.684299	11.714388	5.755712
-796.498031	2.384443	5.765709
-795.146903	6.925656	5.775706
-792.958018	5.933269	5.785702
-791.219341	0.896742	5.795699
-789.232364	4.322707	5.805696
-787.160172	8.117140	5.815693
-785.691010	1.265370	5.825690
-783.714856	5.346718	5.835686
-781.746164	4.905820	5.845683
-779.870729	5.376621	5.855680
-778.014801	1.252894	5.865677
-776.372741	3.699839	5.875674
-774.112385	1.158234	5.885670
-772.487183	-2.527583	5.895667
-770.308539	-3.284641	5.905664
-768.798801	11.727520	5.915661
-766.617403	4.452478	5.925658
-765.057117	8.893973	5.935654
-763.051225	-3.501688	5.945651
-761.065985	10.558221	5.955648
-759.208033	8.671432	5.965645
-757.361814	8.725364	5.975642
-755.661914	5.777578	5.985638
-753.777590	4.361817	5.995635
-751.622779	3.561219	6.005632
-749.927435	2.748789	6.015629
-747.819189	0.534658	6.025626
-746.204998	5.494891	6.035622
-744.415873	-0.492246	6.045619
-742.186489	3.228163	6.055616
-740.503297	6.360103	6.065613
-738.611817	1.772853	6.075610
-736.842468	13.697930	6.085606
-734.812900	3.976254	6.095603
-732.720382	7.650654	6.105600
-731.028855	2.010682	6.115597
-729.067524	9.081658	6.125594
-727.727414	3.316273	6.135590
-725.394057	6.325385	6.145587
-723.848802	6.215868	6.155584
-721.909484	2.827238	6.165581
-719.621216	-0.211381	6.175578
-717.891252	-0.291991	6.185574
-716.065437	5.935432	6.195571
-714.172199	1.681060	6.205568
-712.498691	6.612894	6.215565
-710.326677	0.364083	6.225562
-708.586811	6.243686	6.235558
-706.753058	9.201602	6.245555
-704.856006	6.710218	6.255552
-703.248017	1.129400	6.265549
-701.077355	3.278790	6.275546
-699.371390	3.285707	6.285542
-697.273462	4.540454	6.295539
-695.246968	1.658942	6.305536
-693.607389	-6.388364	6.315533
-691.900268	0.574846	6.325530
-689.825264	2.532700	6.335526
-687.974732	6.143178	6.345523
-685.984685	2.493852	6.355520
-684.141013	0.696241	6.365517
-682.191845	5.303016	6.375514
-680.468763	1.759504	6.385510
-678.304487	4.400962	6.395507
-676.836211	-1.642228	6.405504
-674.907472	8.422794	6.415501
-673.110503	0.632968	6.425498
-671.065589	-1.460457	6.435494
-669.226607	1.731903	6.445491
-667.095033	6.544799	6.455488
-665.529283	-1.539641	6.465485
-663.402109	1.478792	6.475482
-661.842236	-0.076103	6.485478
-659.828050	4.326103	6.495475
-657.851079	4.046608	6.505472
-656.159951	2.968089	6.515469
-654.225928	10.395583	6.525466
-652.017525	12.867395	6.535462
-650.634801	-2.445840	6.545459
-648.749724	-1.409662	6.555456
-646.965825	1.384169	6.565453
-644.563410	5.928039	6.575450
-642.957755	7.484101	6.585446
-641.082564	-2.001270	6.595443
-639.040722	3.787516	6.605440
-637.130187	0.741428	6.615437
-635.449099	3.070139	6.625434
-633.651108	3.135030	6.635430
-631.588087	8.802026	6.645427
-629.984621	-3.191374	6.655424
-627.835820	2.196671	6.665421
-625.736581	10.597219	6.675418
-624.501409	6.534877	6.685414
-622.412675	2.812998	6.695411
-620.583244	1.983975	6.705408
-618.497610	-0.610095	6.715405
-616.868482	8.677097	6.725402
-614.706100	4.829780	6.735398
-612.741498	4.792286	6.745395
-610.937664	2.604798	6.755392
-609.220062	-3.397660	6.765389
-607.308244	2.075627	6.775386
-605.213422	4.232485	6.785382
-603.504147	4.848385	6.795379
-601.651457	3.431480	6.805376
-599.960926	3.170949	6.815373
-597.927649	-1.517789	6.825370
-596.106165	1.667952	6.835366
-594.276619	3.684047	6.845363
-592.234185	-6.180091	6.855360
-590.222031	-3.136902	6.865357
-588.361197	0.522534	6.875354
-586.549293	11.092593	6.885350
-584.722011	-0.374460	6.895347
-582.995907	3.292293	6.905344
-580.828496	0.036278	6.915341
-579.070519	-1.701778	6.925338
-577.354715	-1.884230	6.935334
-575.618740	-4.460304	6.945331
-573.248644	8.289433	6.955328
-571.768490	0.766584	6.965325
-569.998709	5.796826	6.975322
-567.810312	0.436000	6.985318
-565.794623	10.941949	6.995315
-564.363844	6.188427	7.005312
-562.245811	-4.954015	7.015309
-560.006825	9.877100	7.025306
-558.559142	6.522914	7.035302
-556.888573	11.685852	7.045299
-554.616075	0.351381	7.055296
-552.909943	1.866194	7.065293
-550.967321	-1.345996	7.075290
-549.077903	0.248487	7.085286
-547.028440	5.297232	7.095283
-545.445902	8.270139	7.105280
-543.920655	-4.692776	7.115277
-541.612510	13.507670	7.125274
-539.569459	6.431746	7.135270
-537.944854	0.864164	7.145267
-535.902355	11.844258	7.155264
-533.930755	4.271356	7.165261
-532.157491	3.599784	7.175258
-530.463759	12.123609	7.185254
-528.651717	1.715287	7.195251
-526.521240	4.428599	7.205248
-524.442629	1.351017	7.215245
-522.874905	-2.172310	7.225242
-521.026794	2.679679	7.235238
-519.160132	0.267499	7.245235
-517.317153	1.964157	7.255232
-515.412807	4.947266	7.265229
-513.350587	3.727481	7.275226
-511.400199	5.571192	7.285222
-509.966260	10.415132	7.295219
-507.842782	0.954931	7.305216
-505.801174	12.794101	7.315213
-504.148497	5.730025	7.325210
-502.457746	10.769787	7.335206
-500.676055	0.440537	7.345203
-498.253467	4.315058	7.355200
-496.325591	6.348684	7.365197
-494.614366	1.330952	7.375194
-492.661988	6.711025	7.385190
-491.121216	3.000977	7.395187
-489.391122	8.666012	7.405184
-487.204910	1.366753	7.415181
-485.268774	3.376964	7.425178
-483.345202	4.883946	7.435174
-481.531390	0.148246	7.445171
-479.583838	-2.767849	7.455168
-477.677878	-2.600088	7.465165
-476.086784	4.628128	7.475162
-473.887984	1.858221	7.485158
-472.125186	6.067067	7.495155
-470.332883	4.783058	7.505152
-468.215968	1.366265	7.515149
-466.297020	2.922944	7.525146
-464.930683	6.906172	7.535142
-463.085943	3.449166	7.545139
-460.951991	7.455077	7.555136
-458.784007	13.819124	7.565133
-457.269298	-1.202493	7.575130
-455.267822	5.334976	7.585126
-453.659074	9.500545	7.595123
-451.627156	5.506842	7.605120
-449.438361	6.291009	7.615117
-447.660486	6.532928	7.625114
-445.871733	8.697752	7.635110
-444.075577	14.375960	7.645107
-442.424648	1.372496	7.655104
-439.838499	3.991024	7.665101
-438.569734	0.734947	7.675098
-436.688678	11.399880	7.685094
-434.694686	4.052412	7.695091
-432.680282	11.132550	7.705088
-431.189447	7.032636	7.715085
-428.864333	6.301446	7.725082
-426.936976	5.809021	7.735078
-425.628305	7.185295	7.745075
-423.423204	10.878318	7.755072
-421.387815	4.801556	7.765069
-419.521970	5.831515	7.775066
-417.730065	8.715823	7.785062
-415.976143	4.280243	7.795059
-414.068281	7.900738	7.805056
-412.150525	6.372541	7.815053
-410.288085	10.317646	7.825050
-408.356215	10.759206	7.835046
-406.507181	6.930521	7.845043
-404.749227	5.191014	7.855040
-402.732275	7.900461	7.865037
-400.654523	-0.623979	7.875034
-398.914390	1.488646	7.885030
-397.104184	7.701462	7.895027
-395.324445	8.670982	7.905024
-393.369891	4.482845	7.915021
-391.639526	-1.728342	7.925018
-389.627325	2.368121	7.935014
-387.528876	4.453548	7.945011
-385.877350	8.792326	7.955008
-384.166241	7.410822	7.965005
-382.189882	-0.157989	7.975002
-380.221891	8.672678	7.984998
-378.373669	9.138669	7.994995
-376.514698	8.058811	8.004992
-374.697467	6.557744	8.014989
-372.699708	9.663421	8.024986
-370.686418	7.660554	8.034982
-368.813681	10.394634	8.044979
-367.197124	15.402137	8.054976
-365.405830	6.844508	8.064973
-363.366768	12.523474	8.074970
-361.410370	9.953408	8.084966
-359.421621	9.871217	8.094963
-358.018510	8.876778	8.104960
-355.924012	9.155057	8.114957
-353.807813	8.462027	8.124954
-352.324044	5.429024	8.134950
-350.173946	4.924786	8.144947
-348.255131	14.266996	8.154944
-346.479956	2.348959	8.164941
-344.443519	-1.018567	8.174938
-342.458787	7.834724	8.184934
-341.162626	3.739098	8.194931
-338.963644	-1.924787	8.204928
-336.969222	8.305316	8.214925
-335.154015	-3.986977	8.224922
-333.270072	-1.515173	8.234918
-331.704274	5.101430	8.244915
-329.749214	7.740298	8.254912
-327.484788	-1.195970	8.264909
-325.749059	-0.711982	8.274906
-324.077766	-3.054935	8.284902
-322.180551	-3.288266	8.294899
-320.110204	5.054033	8.304896
-318.064226	-2.331641	8.314893
-316.605136	-5.343315	8.324890
-314.501723	-5.293780	8.334886
-312.652222	6.923592	8.344883
-310.769399	-0.663392	8.354880
-308.843405	3.596896	8.364877
-307.046247	-2.809625	8.374874
-305.152295	1.054747	8.384870
-303.550866	5.685779	8.394867
-301.481873	4.277206	8.404864
-299.421238	9.453863	8.414861
-297.606015	2.840788	8.424858
-295.954173	-1.349479	8.434854
-293.874481	0.830599	8.444851
-291.945588	-0.143518	8.454848
-290.327439	5.146401	8.464845
-288.339116	4.925396	8.474842
-286.318789	0.390544	8.484838
-284.533325	-1.309059	8.494835
-282.789211	10.642545	8.504832
-280.575953	2.022361	8.514829
-278.936233	-1.861238	8.524826
-277.183116	8.825836	8.534822
-275.448315	-0.515308	8.544819
-273.492706	-5.993456	8.554816
-270.974875	7.216178	8.564813
-269.337866	-4.635546	8.574810
-267.880855	1.243763	8.584807
-266.027617	-0.989251	8.594803
-264.058180	2.222087	8.604800
-261.771005	-3.877366	8.614797
-259.906026	-4.149711	8.624794
-258.344736	9.427330	8.634791
-256.596941	6.532236	8.644787
-254.392362	-0.521877	8.654784
-252.688694	-0.241130	8.664781
-250.534212	-3.638471	8.674778
-248.737556	-4.376723	8.684775
-247.002309	-1.551134	8.694771
-245.085640	1.117615	8.704768
-242.896043	-7.465601	8.714765
-241.352790	-10.394350	8.724762
-239.711645	-5.870663	8.734759
-237.383911	-7.773609	8.744755
-235.683962	-5.196578	8.754752
-234.079015	-0.905517	8.764749
-232.272151	-6.951973	8.774746
-230.011132	-4.456583	8.784743
-228.184859	3.100583	8.794739
-226.499780	-1.042841	8.804736
-224.392739	0.645063	8.814733
-222.762098	-1.893432	8.824730
-221.159602	-4.683210	8.834727
-218.981920	6.626125	8.844723
-217.014818	2.200869	8.854720
-215.025117	-2.076419	8.864717
-213.052486	-3.748999	8.874714
-211.348380	-3.304089	8.884711
-209.684843	-0.236513	8.894707
-207.583946	-8.450299	8.904704
-205.660377	-6.761521	8.914701
-203.848316	-7.814814	8.924698
-201.881654	-16.131901	8.934695
-200.287916	-10.167006	8.944691
-198.210720	-4.321885	8.954688
-196.417414	-3.788572	8.964685
-194.760206	-10.467931	8.974682
-192.741469	-5.467646	8.984679
-190.738571	-3.412584	8.994675
-188.868503	-7.386563	9.004672
-186.872196	3.520713	9.014669
-185.036866	-4.172283	9.024666
-183.040547	-4.236591	9.034663
-181.690365	-3.100478	9.044659
-179.414185	-5.056720	9.054656
-177.364585	-1.059192	9.064653
-175.856655	-2.043411	9.074650
-174.133449	3.334035	9.084647
-171.895683	2.113368	9.094643
-170.039530	-1.225251	9.104640
-168.387029	-1.488884	9.114637
-166.483380	-5.545571	9.124634
-164.275667	-6.433029	9.134631
-162.766256	-4.521825	9.144627
-160.530129	-0.506677	9.154624
-158.897850	-4.306911	9.164621
-156.842355	4.749985	9.174618
-155.095362	0.239903	9.184615
-153.154808	-4.214223	9.194611
-151.406381	13.720738	9.204608
-149.523933	0.440504	9.214605
-147.429173	-1.906743	9.224602
-145.639053	3.292688	9.234599
-143.963370	7.648315	9.244595
-141.925092	3.879624	9.254592
-140.117332	2.103938	9.264589
-138.499138	7.761840	9.274586
-136.187777	7.653622	9.284583
-134.456431	-2.184229	9.294579
-132.596808	10.896916	9.304576
-130.694801	-2.149593	9.314573
-128.713137	-0.831582	9.324570
-127.022881	3.869084	9.334567
-125.259994	10.253876	9.344563
-123.209558	4.465458	9.354560
-121.105704	4.941387	9.364557
-119.405058	-1.039103	9.374554
-117.591203	-0.526377	9.384551
-115.712694	0.266549	9.394547
-113.865221	0.249728	9.404544
-112.155820	2.015381	9.414541
-110.045629	0.526190	9.424538
-108.350729	-1.438299	9.434535
-106.248109	3.727097	9.444531
-104.302701	-0.838289	9.454528
-102.446292	3.038556	9.464525
-100.611515	-2.008101	9.474522
-99.023797	-0.988780	9.484519
-96.852243	3.087256	9.494515
-95.114088	7.052444	9.504512
-93.116305	5.642776	9.514509
-91.199683	-2.892035	9.524506
-89.690871	2.443892	9.534503
-87.496235	-7.343104	9.544499
-86.001842	-7.104639	9.554496
-83.855264	-0.463674	9.564493
-81.695144	-3.234958	9.574490
-79.655899	1.607429	9.584487
-78.298519	-2.846763	9.594483
-76.399851	-2.267014	9.604480
-74.422275	-4.549718	9.614477
-72.479689	0.794388	9.624474
-70.688513	5.963712	9.634471
-68.731560	-3.008549	9.644467
-67.083023	1.005690	9.654464
-64.832311	5.072287	9.664461
-63.107898	-2.647142	9.674458
-61.341453	5.803879	9.684455
-59.553040	6.795949	9.694451
-57.640645	4.185774	9.704448
-55.823232	0.615008	9.714445
-53.528395	-0.472556	9.724442
-51.722633	-1.040019	9.734439
-50.087302	3.659993	9.744435
-48.117494	5.155218	9.754432
-46.198150	2.095543	9.764429
-44.365857	4.470036	9.774426
-42.532884	4.624522	9.784423
-40.559607	1.036799	9.794419
-38.882256	-1.216936	9.804416
-36.859017	8.015740	9.814413
-34.965134	8.163674	9.824410
-33.001062	0.273410	9.834407
-31.417325	-1.251737	9.844403
-29.568834	0.234434	9.854400
-27.399409	-0.529958	9.864397
-25.171584	-4.966653	9.874394
-23.832067	-1.149398	9.884391
-22.021433	-3.561743	9.894387
-20.157480	6.638943	9.904384
-18.106317	2.257270	9.914381
-16.543921	2.630188	9.924378
-14.027098	1.625670	9.934375
-12.356136	5.884257	9.944371
-10.915160	10.968967	9.954368
-8.830964	-1.471816	9.964365
-6.824364	-6.863165	9.974362
-5.080384	-4.982956	9.984359
-3.871944	25.746655	9.994355
-2.522796	53.390859	10.004352
-1.189217	114.473684	10.014349
0.000000	160.029397	10.019354
0.431999	207.561703	10.024359
0.894244	227.675226	10.029363
1.468493	269.509852	10.034368
1.257871	295.569998	10.039373
2.275122	318.993327	10.044378
2.360736	344.090139	10.049383
2.882134	348.214157	10.054387
2.948192	361.220916	10.059392
2.691781	387.938212	10.064397
3.130830	385.537552	10.069402
3.047224	386.027131	10.074407
3.028445	397.505246	10.079411
3.257578	412.524974	10.084416
3.597554	422.804214	10.089421
3.886195	431.104750	10.094426
3.764010	437.283647	10.099431
3.499318	442.185905	10.104435
3.773300	445.701304	10.109440
3.481351	445.274817	10.114445
3.872592	435.553896	10.119450
3.604730	444.033080	10.124455
3.840377	445.504617	10.129459
3.762187	457.421173	10.134464
3.560334	457.918576	10.139469
3.541296	451.382202	10.144474
3.743037	478.457089	10.149479
4.111670	482.130861	10.154483
4.234273	484.317425	10.159488
4.181711	489.307288	10.164493
4.470240	490.417167	10.169498
4.490527	495.469528	10.174503
4.291479	497.849317	10.179507
4.551205	497.199227	10.184512
4.180033	501.457761	10.189517
4.787005	492.508197	10.194522
4.340229	503.334010	10.199527
4.480648	505.522466	10.204531
5.000216	506.295885	10.209536
4.647550	505.828618	10.214541
4.765613	502.622871	10.219546
4.688329	511.939000	10.224551
4.525173	513.929877	10.229555
5.048293	515.458071	10.234560
4.869703	521.199733	10.239565
5.036633	511.443576	10.244570
4.721661	511.536409	10.249575
4.863074	514.674010	10.254579
4.939535	507.012233	10.259584
4.645282	523.569465	10.264589
4.779365	530.450256	10.269594
4.864327	547.948375	10.274599
4.899104	546.996700	10.279603
4.848223	544.532231	10.284608
5.023781	552.380952	10.289613
4.972142	542.473558	10.294618
5.181417	574.090518	10.299623
5.394090	577.243574	10.304627
5.198731	578.941558	10.309632
5.189393	582.249870	10.314637
5.442391	586.886687	10.319642
5.622909	585.995342	10.324647
5.511970	594.763393	10.329651
5.613847	593.996552	10.334656
5.625026	596.894749	10.339661
5.838292	589.334110	10.344666
5.695548	598.435236	10.349671
5.913517	613.199915	10.354675
6.416301	621.007522	10.359680
6.398494	624.875426	10.364685
6.061215	608.450383	10.369690
5.974010	604.574044	10.374695
6.050812	606.212854	10.379699
6.105448	605.850931	10.384704
5.905951	613.816272	10.389709
6.535721	613.286928	10.394714
6.491366	640.201098	10.399719
6.312926	635.894608	10.404723
6.657758	629.013120	10.409728
6.430202	627.951895	10.414733
6.515864	621.075476	10.419738
6.133055	624.550594	10.424743
6.297342	634.753929	10.429747
6.620174	644.026829	10.434752
6.622771	651.338649	10.439757
6.708940	640.013628	10.444762
6.774756	647.253863	10.449767
6.656797	656.841496	10.454771
6.808546	654.138114	10.459776
6.742600	649.955602	10.464781
6.921373	645.574791	10.469786
6.659824	659.204915	10.474791
6.561483	648.883857	10.479795
6.735778	658.650380	10.484800
6.846684	669.973989	10.489805
7.440044	673.078967	10.494810
7.260277	676.917523	10.499815
7.093042	704.717145	10.504819
7.273550	690.346173	10.509824
7.326101	689.462616	10.514829
7.306124	681.893398	10.519834
7.186963	693.301026	10.524839
7.585399	694.784472	10.529843
7.387119	692.313525	10.534848
7.381399	690.138292	10.539853
7.587935	682.961873	10.544858
7.463053	695.676114	10.549863
7.336670	691.028572	10.554867
7.688343	693.419904	10.559872
7.446483	695.622051	10.564877
7.416838	687.975526	10.569882
7.724425	706.852839	10.574887
7.951842	722.032433	10.579891
8.491975	718.666283	10.584896
8.044602	709.514164	10.589901
8.125255	691.822324	10.594906
7.871698	690.885087	10.599911
7.855669	701.877310	10.604915
8.325544	720.288792	10.609920
8.160631	724.935537	10.614925
8.545754	725.733566	10.619930
8.413221	737.766251	10.624935
8.260247	709.596636	10.629939
8.571594	709.280499	10.634944
8.402470	716.624470	10.639949
8.343852	708.700283	10.644954
8.159214	727.279240	10.649959
8.419444	736.920148	10.654963
8.751711	729.450843	10.659968
8.434460	729.301192	10.664973
8.562186	722.504749	10.669978
8.800524	737.092843	10.674983
8.625304	736.493189	10.679987
8.932239	735.499672	10.684992
8.753570	742.580253	10.689997
8.959532	741.184952	10.695002
8.795504	734.671575	10.700007
8.584207	728.604128	10.705011
8.822011	741.547568	10.710016
9.031704	750.452231	10.715021
8.978454	741.756047	10.720026
8.931435	748.162782	10.725031
9.150734	764.602112	10.730035
9.289753	765.237546	10.735040
9.199379	775.976755	10.740045
9.475720	763.664104	10.745050
9.698957	774.138832	10.750055
9.616384	773.057625	10.755059
9.632410	755.114243	10.760064
9.200644	750.534310	10.765069
9.727835	764.330471	10.770074
9.533557	781.561174	10.775079
9.644861	782.467532	10.780083
9.486567	780.762894	10.785088
9.548635	781.413755	10.790093
9.676903	777.479350	10.795098
9.839171	789.521830	10.800103
9.700190	785.552776	10.805107
9.885705	788.142511	10.810112
9.950845	787.821486	10.815117
10.001476	782.484944	10.820122
9.776708	775.963889	10.825127
9.899089	776.040586	10.830131
10.518638	776.301339	10.835136
10.179602	782.157001	10.840141
10.270248	775.095213	10.845146
10.203773	787.663026	10.850151
9.879847	791.486757	10.855155
10.155067	789.465398	10.860160
10.281144	788.850804	10.865165
10.392809	795.347368	10.870170
10.350515	806.865828	10.875175
10.422353	817.257500	10.880179
10.878107	806.765956	10.885184
10.582690	818.931919	10.890189
10.927477	810.908645	10.895194
10.987150	804.145094	10.900199
10.752795	796.193693	10.905203
10.530873	793.948848	10.910208
10.399166	807.181513	10.915213
10.846913	802.686795	10.920218
10.791356	807.301932	10.925223
10.813254	809.914613	10.930227
11.009258	815.022639	10.935232
10.954236	818.827144	10.940237
11.104495	820.843770	10.945242
11.024537	821.933598	10.950247
10.935988	817.633217	10.955251
11.162053	812.782769	10.960256
11.263539	810.159914	10.965261
11.364622	813.056432	10.970266
11.311179	827.967119	10.975271
11.068373	826.684383	10.980275
11.565743	818.182609	10.985280
10.891926	823.233823	10.990285
11.473257	838.458019	10.995290
11.617898	851.441647	11.000295
11.591432	843.885995	11.005299
11.693370	854.077351	11.010304
11.529904	856.524062	11.015309
11.651600	855.186344	11.020314
11.658847	854.226424	11.025319
11.491968	854.481718	11.030323
11.731697	855.927416	11.035328
11.529420	865.637444	11.040333
11.458385	863.024748	11.045338
11.830693	864.846694	11.050343
12.158692	871.220481	11.055347
12.727756	869.451867	11.060352
12.140273	867.628011	11.065357
12.291461	864.557250	11.070362
12.186615	849.361154	11.075367
12.360175	847.982050	11.080371
12.391895	840.620545	11.085376
12.147711	846.331796	11.090381
12.580515	866.941339	11.095386
12.802581	863.244263	11.100391
12.787516	854.366879	11.105395
12.401102	851.004971	11.110400
12.498008	865.139512	11.115405
12.966782	852.113276	11.120410
12.857058	859.033108	11.125415
12.536660	858.727838	11.130419
12.541615	847.742037	11.135424
12.603132	859.046862	11.140429
13.175602	874.209432	11.145434
13.153697	862.196577	11.150439
12.654415	861.722717	11.155443
12.858784	852.933340	11.160448
13.362294	868.272481	11.165453
13.149747	867.768661	11.170458
13.068449	859.843277	11.175463
12.733757	859.105048	11.180467
13.216905	858.662161	11.185472
13.353659	877.462865	11.190477
13.151756	875.558589	11.195482
13.321657	873.590286	11.200487
13.322504	877.419012	11.205491
13.411463	885.188685	11.210496
13.031541	884.257396	11.215501
13.829838	877.555783	11.220506
13.475016	879.089998	11.225511
13.492957	892.606380	11.230515
13.558725	882.746260	11.235520
13.652144	884.986425	11.240525
13.789693	884.176033	11.245530
13.656797	880.797339	11.250535
13.869756	882.311964	11.255539
13.952991	875.437389	11.260544
13.563680	882.594210	11.265549
13.785959	890.850403	11.270554
14.029658	881.376645	11.275559
13.665322	888.736067	11.280563
13.855961	899.525168	11.285568
14.378278	906.009905	11.290573
14.502780	907.787800	11.295578
14.447300	893.876887	11.300583
14.515739	883.650487	11.305587
14.614153	879.550505	11.310592
14.160361	883.773440	11.315597
14.445842	877.264001	11.320602
14.430527	873.674168	11.325607
14.478308	883.703873	11.330611
14.461157	890.258871	11.335616
14.112163	887.868697	11.340621
14.298159	897.103661	11.345626
14.535144	919.893899	11.350631
14.657344	917.797579	11.355635
14.873419	906.002200	11.360640
14.773857	915.930846	11.365645
14.725607	908.244593	11.370650
14.825944	909.821338	11.375655
14.728143	918.308367	11.380659
15.348831	909.515636	11.385664
15.171778	925.179423	11.390669
15.103302	913.777927	11.395674
14.850454	917.882091	11.400679
14.969084	919.966853	11.405683
15.371877	900.159145	11.410688
15.036904	914.564464	11.415693
15.123942	909.293032	11.420698
15.267029	913.594247	11.425703
15.073707	907.273122	11.430707
15.331517	914.467101	11.435712
14.975412	915.484283	11.440717
15.421991	915.238039	11.445722
15.487509	926.619550	11.450727
15.572440	945.403376	11.455731
16.011223	933.656034	11.460736
15.683750	930.559097	11.465741
15.839271	902.521255	11.470746
15.554116	919.984236	11.475751
15.806301	920.975367	11.480755
16.041735	920.349635	11.485760
15.810491	922.397157	11.490765
16.137363	918.221304	11.495770
15.939904	918.167662	11.500775
15.596418	912.334108	11.505779
16.038405	927.638971	11.510784
15.995080	939.490439	11.515789
16.158168	941.713194	11.520794
16.284516	944.378627	11.525799
16.314423	949.584155	11.530803
16.245288	930.589688	11.535808
16.319774	950.472750	11.540813
16.539725	937.719512	11.545818
16.656908	944.453384	11.550823
16.472348	942.035399	11.555827
17.091307	935.874874	11.560832
16.418759	927.916015	11.565837
16.373536	918.097226	11.570842
16.713454	937.108458	11.575847
16.716075	938.249780	11.580851
16.693463	933.443683	11.585856
16.820435	947.436315	11.590861
16.862409	952.766076	11.595866
16.843525	947.219786	11.600871
16.629070	952.054277	11.605875
16.898032	931.310655	11.610880
16.580715	945.957618	11.615885
16.822243	948.371292	11.620890
16.899109	943.787448	11.625895
16.817835	946.867618	11.630899
16.887031	948.994962	11.635904
17.057572	948.518351	11.640909
17.279027	939.622116	11.645914
16.725076	942.186311	11.650919
16.687773	980.501411	11.655923
17.408557	955.057309	11.660928
17.301149	975.642777	11.665933
17.196749	981.852184	11.670938
17.474578	975.902168	11.675943
17.545494	970.516589	11.680947
18.058587	970.136734	11.685952
17.633057	978.155669	11.690957
17.871729	975.081971	11.695962
17.859078	967.454665	11.700967
17.811673	967.079045	11.705971
18.100346	966.790175	11.710976
17.866817	968.612562	11.715981
17.988321	952.847244	11.720986
17.906490	980.086569	11.725991
17.970062	977.237917	11.730995
18.274536	960.372651	11.736000
18.036573	972.594235	11.741005
17.783488	978.275417	11.746010
18.184512	964.841990	11.751015
17.777113	966.250557	11.756019
17.789401	969.926095	11.761024
17.869707	972.403333	11.766029
18.257230	961.018962	11.771034
18.106149	988.867016	11.776039
18.405862	1001.305649	11.781043
18.661719	988.152399	11.786048
18.400750	984.913955	11.791053
18.685177	992.288233	11.796058
18.555253	992.988647	11.801063
18.511651	973.349805	11.806067
18.353686	1001.810843	11.811072
18.707890	991.822646	11.816077
19.000375	983.306144	11.821082
19.031270	984.561232	11.826087
19.213192	995.071095	11.831091
19.036206	977.489382	11.836096
18.858766	999.868022	11.841101
19.169274	993.498045	11.846106
19.301873	986.697547	11.851111
19.024723	992.019870	11.856115
19.461186	978.896172	11.861120
19.449834	987.708502	11.866125
19.310428	969.639831	11.871130
19.081799	965.262397	11.876135
19.361140	985.253186	11.881139
19.724212	977.786726	11.886144
18.970091	968.222889	11.891149
19.134004	977.792588	11.896154
19.771618	982.658356	11.901159
19.376422	988.887336	11.906163
19.683931	990.744864	11.911168
19.573779	997.078199	11.916173
19.776326	993.519823	11.921178
19.480928	990.898731	11.926183
19.377006	998.838000	11.931187
19.460989	977.336908	11.936192
19.550602	1006.212636	11.941197
19.742646	992.795166	11.946202
19.801493	978.698780	11.951207
19.754815	989.491104	11.956211
19.777146	986.541794	11.961216
20.031305	990.689699	11.966221
20.238472	1003.450603	11.971226
20.116307	1008.347665	11.976231
20.357950	1008.145144	11.981235
20.261640	989.821990	11.986240
20.277173	1009.443297	11.991245
20.084976	1002.634667	11.996250
20.093652	1009.327527	12.001255
20.331981	1021.509461	12.006259
20.630944	1014.228251	12.011264
20.427524	1015.832951	12.016269
20.439623	1017.340201	12.021274
20.510184	1014.949325	12.026279
20.383590	1010.601337	12.031283
20.280547	1023.343922	12.036288
20.585015	1023.675435	12.041293
20.447596	1009.958829	12.046298
20.604340	1000.938836	12.051303
20.878337	1021.668547	12.056307
20.643876	1027.349932	12.061312
20.669558	1027.913566	12.066317
20.788119	1015.384590	12.071322
20.836836	1022.772821	12.076327
20.275946	1007.600404	12.081331
20.724244	986.369205	12.086336
20.444981	978.934224	12.091341
20.606047	985.456112	12.096346
20.584776	982.297713	12.101351
20.591793	996.415181	12.106355
20.563965	978.647250	12.111360
20.345981	969.182411	12.116365
20.271371	1002.659092	12.121370
20.321712	971.996471	12.126375
20.359096	1023.555731	12.131379
21.175735	1003.858500	12.136384
20.794503	991.377714	12.141389
20.574535	987.372633	12.146394
20.471097	995.803836	12.151399
20.546457	984.913935	12.156403
20.858486	986.064263	12.161408
20.333193	999.181677	12.166413
20.518439	982.567214	12.171418
20.370091	990.318021	12.176423
20.234337	1002.305707	12.181427
20.573963	993.548290	12.186432
20.744302	990.930191	12.191437
20.090910	988.279461	12.196442
20.672448	989.754239	12.201447
20.409571	993.082580	12.206451
20.764246	987.298500	12.211456
20.382295	991.863248	12.216461
20.527352	991.959985	12.221466
20.631448	992.757118	12.226471
20.490791	1001.128028	12.231475
20.381786	993.448265	12.236480
20.335741	992.236636	12.241485
20.314060	988.472746	12.246490
20.267643	991.506366	12.251495
20.578481	1014.095740	12.256499
21.111299	1007.166749	12.261504
20.528814	1002.621809	12.266509
20.619592	986.779351	12.271514
20.486781	999.216001	12.276519
20.265134	996.527952	12.281523
20.475551	988.410892	12.286528
20.280324	989.873933	12.291533
20.507829	990.228758	12.296538
20.840493	993.249230	12.301543
20.638241	1004.127878	12.306547
20.713516	989.686659	12.311552
20.371300	1004.000181	12.316557
20.757449	993.480181	12.321562
20.807936	1003.096372	12.326567
20.769705	1004.772498	12.331571
20.929359	998.707277	12.336576
20.351781	1001.455023	12.341581
20.932559	995.492954	12.346586
20.894776	1009.989743	12.351591
20.695177	1005.803211	12.356595
20.900057	993.804541	12.361600
20.190042	977.537869	12.366605
20.256894	973.403470	12.371610
20.438257	982.308065	12.376615
20.478076	994.586291	12.381619
20.845101	1001.997864	12.386624
20.788735	999.242454	12.391629
20.642241	985.774902	12.396634
20.567925	986.898536	12.401639
20.257838	986.895971	12.406643
20.465659	977.803190	12.411648
20.393457	987.997184	12.416653
20.242013	979.575138	12.421658
20.591253	991.841861	12.426663
20.259828	1006.987879	12.431667
20.628933	1003.883912	12.436672
20.609202	1009.438003	12.441677
20.633270	1001.401118	12.446682
20.678096	987.685431	12.451687
20.493932	980.976456	12.456691
20.751342	977.748381	12.461696
20.400768	992.452734	12.466701
20.272973	981.335037	12.471706
20.413400	979.857125	12.476711
20.372367	991.914852	12.481715
20.815905	997.530673	12.486720
20.765889	992.517614	12.491725
20.524048	989.746054	12.496730
20.652396	983.250589	12.501735
20.353357	991.053814	12.506739
20.576795	981.616339	12.511744
20.739977	982.478166	12.516749
20.305748	982.799754	12.521754
20.550636	971.543779	12.526759
20.205865	986.048504	12.531763
20.703554	984.478920	12.536768
20.672349	980.418505	12.541773
20.785064	974.292971	12.546778
20.405906	984.444453	12.551783
20.182460	980.801053	12.556787
20.338994	980.690954	12.561792
20.478965	982.357580	12.566797
20.493120	986.885963	12.571802
20.740643	979.001112	12.576807
20.571899	979.609945	12.581811
20.426254	978.355854	12.586816
20.506413	977.376412	12.591821
20.316166	993.384578	12.596826
20.487177	981.156351	12.601831
20.422129	982.964485	12.606835
20.975355	973.338801	12.611840
20.600901	1004.589326	12.616845
20.739087	1000.371002	12.621850
21.167670	984.466788	12.626855
20.959098	985.285402	12.631859
20.894535	991.267685	12.636864
21.000588	991.555147	12.641869
20.711050	975.142571	12.646874
20.760040	958.799026	12.651879
19.924529	965.774736	12.656883
20.384839	958.250201	12.661888
20.285525	987.431991	12.666893
20.409747	985.961394	12.671898
20.828214	986.610618	12.676903
20.420642	996.859681	12.681907
20.587246	998.673450	12.686912
20.697167	998.007808	12.691917
20.352740	977.626876	12.696922
20.581366	999.601708	12.701927
20.296993	986.410037	12.706931
20.745147	992.395707	12.711936
20.707879	976.658838	12.716941
20.309442	963.248835	12.721946
20.625879	973.674151	12.726951
20.379767	979.827311	12.731955
20.636270	985.335760	12.736960
20.407310	971.638522	12.741965
20.375770	992.629809	12.746970
20.669878	979.205537	12.751975
20.272171	992.917613	12.756979
20.385610	985.694390	12.761984
20.476126	993.567954	12.766989
20.643638	996.460223	12.771994
20.396993	992.375816	12.776999
20.401828	1004.889866	12.782003
20.503163	992.688512	12.787008
20.538419	997.153607	12.792013
20.500551	1001.961529	12.797018
20.775069	997.355607	12.802023
20.416496	1009.454530	12.807027
20.774558	998.536879	12.812032
20.613968	1001.517746	12.817037
20.432165	982.642105	12.822042
20.307068	984.617513	12.827047
20.415025	990.610129	12.832051
20.573395	1003.670553	12.837056
20.603495	1012.268128	12.842061
20.809734	1008.026332	12.847066
20.771417	974.242837	12.852071
20.804773	984.041521	12.857075
20.962131	964.274446	12.862080
20.701755	966.266695	12.867085
20.584442	973.630918	12.872090
20.691877	966.913291	12.877095
20.746639	968.823742	12.882099
20.843563	968.215368	12.887104
20.524081	976.310429	12.892109
20.275266	976.742796	12.897114
20.641615	970.450656	12.902119
20.725891	976.732473	12.907123
20.440779	976.934085	12.912128
20.523309	967.452859	12.917133
20.590633	969.965283	12.922138
20.525074	975.003118	12.927143
20.539612	972.815150	12.932147
20.883074	954.565407	12.937152
20.417350	960.881317	12.942157
20.480119	965.386170	12.947162
20.723999	954.431569	12.952167
20.695721	963.117273	12.957171
20.615213	947.850958	12.962176
20.316853	943.579269	12.967181
20.220761	933.516269	12.972186
20.236310	955.569172	12.977191
20.475796	975.815464	12.982195
20.744971	970.713659	12.987200
20.592370	979.999523	12.992205
20.532615	962.742908	12.997210
20.744467	962.270747	13.002215
20.416688	963.300761	13.007219
20.436092	937.785620	13.012224
20.497548	963.917115	13.017229
20.454962	947.646536	13.022234
20.502549	975.155373	13.027239
20.491335	981.304187	13.032243
20.856100	963.913634	13.037248
20.327907	956.881066	13.042253
20.301545	954.073571	13.047258
20.615021	959.166068	13.052263
20.443120	978.058707	13.057267
20.400388	979.189919	13.062272
20.348703	988.978515	13.067277
20.400923	977.559296	13.072282
20.588522	989.287243	13.077287
20.630295	976.516655	13.082291
20.553299	979.246064	13.087296
20.724113	982.044763	13.092301
20.315477	975.497747	13.097306
20.637274	972.891766	13.102311
20.450550	979.879129	13.107315
20.455560	979.856274	13.112320
20.419157	992.261772	13.117325
20.547142	986.316726	13.122330
20.675598	979.658819	13.127335
20.495515	980.266306	13.132339
20.743671	973.877896	13.137344
20.372807	978.825651	13.142349
20.398431	980.704480	13.147354
20.909600	983.256508	13.152359
20.136020	984.758170	13.157363
20.858053	981.993739	13.162368
20.322609	977.357726	13.167373
20.368040	973.769218	13.172378
20.473655	983.310372	13.177383
20.634631	992.423230	13.182387
20.769306	978.797301	13.187392
20.558628	979.125815	13.192397
20.364939	959.848396	13.197402
20.846860	947.808734	13.202407
20.369972	955.085213	13.207411
20.162841	953.721082	13.212416
20.295177	960.819978	13.217421
20.736515	985.723976	13.222426
20.791959	976.783231	13.227431
20.174549	969.930467	13.232435
20.586195	972.323322	13.237440
20.676317	978.339278	13.242445
20.851584	968.253477	13.247450
20.606064	961.237327	13.252455
20.178790	971.885331	13.257459
20.121127	968.641275	13.262464
20.581021	972.792634	13.267469
20.689208	983.345788	13.272474
20.717557	966.368433	13.277479
20.197077	966.058799	13.282483
20.625402	961.587632	13.287488
20.529450	954.995488	13.292493
20.708667	968.378987	13.297498
20.640636	959.979919	13.302503
20.189208	965.498763	13.307507
20.941963	951.775863	13.312512
20.316328	968.430605	13.317517
20.535493	964.240378	13.322522
20.564076	953.045723	13.327527
20.321210	969.007059	13.332531
20.658254	959.255011	13.337536
20.385969	955.974223	13.342541
20.274823	963.812123	13.347546
20.477305	964.035320	13.352551
20.541760	980.714060	13.357555
20.675779	976.673027	13.362560
20.583647	969.200322	13.367565
20.381897	967.046849	13.372570
20.459950	963.121980	13.377575
20.235274	968.705586	13.382579
20.703260	977.777357	13.387584
20.677470	991.285036	13.392589
20.490550	978.934122	13.397594
20.676747	964.560394	13.402599
20.524342	957.594050	13.407603
20.437597	961.596041	13.412608
20.365483	972.884422	13.417613
20.329345	968.933607	13.422618
20.675193	967.932294	13.427623
20.452850	966.299349	13.432627
20.643275	982.336678	13.437632
20.825585	967.715983	13.442637
20.462811	968.997584	13.447642
20.314123	961.309974	13.452647
20.380430	972.727667	13.457651
20.535316	973.885709	13.462656
20.403198	980.362889	13.467661
20.235036	987.454529	13.472666
20.623879	987.580195	13.477671
20.501546	1001.320901	13.482675
20.565441	996.758032	13.487680
20.563817	993.285835	13.492685
20.559556	997.490726	13.497690
20.542772	998.579953	13.502695
20.618561	988.267151	13.507699
20.427639	969.706797	13.512704
20.378750	977.712972	13.517709
20.412852	1004.790351	13.522714
21.176371	988.261854	13.527719
20.578392	975.284213	13.532723
20.454424	989.048823	13.537728
20.426818	974.625604	13.542733
20.468564	974.167956	13.547738
20.428479	960.243485	13.552743
20.330429	970.329624	13.557747
20.522117	980.771687	13.562752
20.513054	986.115908	13.567757
20.627663	986.938174	13.572762
20.731952	966.580312	13.577767
20.409460	973.098889	13.582771
20.598080	972.236193	13.587776
20.688901	979.647650	13.592781
20.601190	975.295048	13.597786
20.679127	964.182400	13.602791
20.655894	978.724146	13.607795
20.819944	967.225599	13.612800
20.573162	985.439480	13.617805
20.480264	981.581294	13.622810
20.779331	972.917091	13.627815
20.631130	973.081097	13.632819
20.773461	962.581081	13.637824
20.741152	990.875401	13.642829
20.415330	961.941223	13.647834
20.655806	991.732732	13.652839
21.036215	977.638679	13.657843
20.865614	949.152860	13.662848
20.583884	956.500718	13.667853
20.409630	944.595670	13.672858
20.570242	961.623330	13.677863
20.503443	932.949099	13.682867
20.751592	937.615190	13.687872
20.384548	929.413640	13.692877
20.207881	945.708170	13.697882
20.462674	943.989671	13.702887
20.021396	951.312509	13.707891
20.101393	960.395684	13.712896
20.163802	970.355307	13.717901
20.409623	978.547871	13.722906
20.569844	977.759089	13.727911
20.178582	991.525330	13.732915
20.553742	980.472501	13.737920
20.515429	981.046339	13.742925
20.438517	977.512036	13.747930
20.616245	972.289196	13.752935
20.518152	979.984673	13.757939
20.687497	976.417403	13.762944
20.512580	981.471104	13.767949
20.519453	976.169855	13.772954
20.727050	973.552125	13.777959
20.270840	988.771643	13.782963
20.411552	981.950929	13.787968
20.797936	979.667387	13.792973
20.346041	971.165529	13.797978
20.744529	982.449827	13.802983
20.371494	973.506457	13.807987
21.039482	990.040068	13.812992
20.681021	973.740988	13.817997
20.634105	973.847840	13.823002
20.918874	991.756181	13.828007
20.551127	951.482451	13.833011
20.283359	960.994829	13.838016
20.634065	959.995896	13.843021
20.634605	954.471735	13.848026
20.668861	937.135503	13.853031
20.515575	948.685970	13.858035
20.730711	950.600803	13.863040
20.200988	955.704773	13.868045
20.347784	958.075210	13.873050
20.316446	955.443550	13.878055
20.514117	971.547521	13.883059
20.931694	973.545190	13.888064
20.506911	958.327463	13.893069
20.175338	950.380442	13.898074
20.531135	947.803737	13.903079
20.504467	963.867783	13.908083
20.491308	959.465449	13.913088
20.499701	959.224434	13.918093
20.592174	965.359859	13.923098
20.451236	954.518669	13.928103
20.412622	965.366460	13.933107
21.029403	971.124953	13.938112
20.515578	954.593628	13.943117
20.410079	964.920649	13.948122
20.735737	954.009776	13.953127
20.244250	962.543849	13.958131
20.515070	952.494859	13.963136
20.633533	942.569524	13.968141
20.164112	950.805179	13.973146
20.570961	953.102602	13.978151
20.234911	956.847883	13.983155
20.480447	971.608534	13.988160
20.964676	973.253372	13.993165
20.705171	962.880521	13.998170
20.669676	953.047541	14.003175
20.449202	957.173362	14.008179
20.819601	952.109036	14.013184
20.865113	956.990378	14.018189
20.362635	948.248346	14.023207
20.320967	971.190032	14.028224
20.275898	952.768689	14.033242
20.657233	945.629675	14.038259
20.550538	967.943113	14.043277
20.528628	968.292676	14.048295
20.753650	955.618246	14.053312
20.440771	954.924167	14.058330
20.471696	965.805565	14.063347
20.749092	955.790487	14.068365
20.417921	963.226699	14.073383
20.803551	970.389730	14.078400
20.703498	977.743474	14.083418
20.560739	955.546921	14.088435
20.694206	998.350536	14.093453
20.803220	987.621435	14.098471
21.206989	983.217316	14.103488
20.564151	972.002552	14.108506
20.617433	997.974349	14.113523
20.984687	997.481667	14.118541
20.801231	992.878631	14.123559
21.160191	993.936621	14.128576
20.638300	991.655743	14.133594
20.937153	1002.993062	14.138611
21.171230	994.960483	14.143629
20.989346	996.543579	14.148647
21.099393	990.369554	14.153664
20.472216	997.046072	14.158682
21.087879	964.153659	14.163699
21.177741	1014.269007	14.168717
20.979984	981.144506	14.173735
20.766034	1011.726768	14.178752
20.866988	986.277775	14.183770
20.613776	1015.142362	14.188787
20.529621	995.961174	14.193805
20.407892	1003.106041	14.198823
20.948700	1017.527076	14.203840
20.762096	1020.141207	14.208858
21.107520	1041.707859	14.213875
21.125963	1006.623533	14.218893
21.104319	1012.690705	14.223911
21.176693	1031.770023	14.228928
20.717706	1014.971832	14.233946
21.038262	1028.924663	14.238963
21.610958	1014.621787	14.243981
21.430951	1037.842030	14.248999
21.576495	1009.711875	14.254016
21.399427	1048.064969	14.259034
21.287921	1020.133083	14.264051
21.127920	1044.869613	14.269069
21.173604	1001.562303	14.274087
21.423658	1026.856291	14.279104
21.446216	1007.571556	14.284122
21.473353	1033.984866	14.289139
21.610166	1011.740493	14.294157
20.968435	1047.809850	14.299175
21.748843	1015.029468	14.304192
21.899249	1060.325254	14.309210
21.804650	1017.793712	14.314227
21.818999	1036.652641	14.319245
21.561524	1005.871861	14.324263
21.510540	1046.600437	14.329280
21.172775	1024.851709	14.334298
21.632305	995.944803	14.339315
21.536290	987.386030	14.344333
21.601045	1004.544393	14.349351
21.921789	1028.008786	14.354368
21.759036	1078.947971	14.359386
21.518484	1054.352383	14.364403
21.823200	1033.551907	14.369421
21.749018	1067.808422	14.374439
21.428051	1062.226898	14.379456
21.660905	1057.272743	14.384474
21.672362	1071.944988	14.389491
22.143435	1036.569761	14.394509
21.544566	1084.813280	14.399527
21.961015	1055.079463	14.404544
21.834274	1053.904257	14.409562
21.890770	1060.317620	14.414579
22.060576	1079.892671	14.419597
21.944467	1058.934341	14.424615
22.572485	1069.763061	14.429632
22.188374	1050.904904	14.434650
22.178368	1066.269518	14.439667
22.364099	1065.388952	14.444685
21.993474	1066.494094	14.449703
22.338330	1053.426105	14.454720
22.207963	1050.398544	14.459738
21.742071	1040.383979	14.464755
22.053525	1063.236461	14.469773
21.902146	1055.320376	14.474791
22.435027	1047.487067	14.479808
22.094268	1064.546587	14.484826
22.206995	1053.088569	14.489843
22.499903	1045.284095	14.494861
22.269360	1061.832129	14.499879
22.269717	1062.719237	14.504896
22.439093	1041.325311	14.509914
22.301848	1063.407826	14.514931
22.606912	1051.875092	14.519949
22.461024	1039.311651	14.524967
22.128993	1066.405188	14.529984
22.244891	1039.125950	14.535002
22.214828	1071.415545	14.540019
22.455033	1030.842373	14.545037
22.102909	1061.449922	14.550055
22.431064	1043.085340	14.555072
22.363879	1059.394969	14.560090
22.314701	1036.179826	14.565107
22.518308	1055.957084	14.570125
22.346133	1048.947192	14.575143
22.422599	1054.482808	14.580160
22.638822	1047.797919	14.585178
22.430333	1052.965295	14.590195
22.772181	1043.234019	14.595213
22.547919	1066.176663	14.600231
22.583825	1047.478030	14.605248
22.577147	1067.592418	14.610266
22.558813	1030.697141	14.615283
22.802290	1074.529445	14.620301
22.980692	1065.168699	14.625319
23.175674	1072.308705	14.630336
22.760138	1053.318710	14.635354
22.599285	1048.740365	14.640371
23.048860	1052.061536	14.645389
22.842961	1053.302420	14.650407
22.988215	1035.407442	14.655424
23.045417	1055.442417	14.660442
23.044744	1037.079950	14.665459
22.893404	1041.344774	14.670477
23.111653	1054.851500	14.675495
22.797067	1051.839161	14.680512
23.064574	1033.556618	14.685530
22.775688	1062.604732	14.690547
23.196531	1044.582425	14.695565
22.974415	1052.031176	14.700583
22.947131	1034.816489	14.705600
23.075973	1054.029969	14.710618
22.701200	1057.743721	14.715635
23.125812	1057.268631	14.720653
22.950931	1064.149884	14.725671
23.266066	1080.205091	14.730688
23.775937	1076.639709	14.735706
23.242021	1070.527454	14.740723
23.277721	1044.796196	14.745741
22.948131	1066.964446	14.750759
23.498037	1055.375359	14.755776
23.310710	1052.959320	14.760794
23.060217	1050.765704	14.765811
23.084736	1072.578627	14.770829
23.330057	1084.240711	14.775847
23.604771	1075.850838	14.780864
23.264598	1092.016860	14.785882
22.919833	1089.437170	14.790899
23.763819	1079.084693	14.795917
23.810083	1085.089158	14.800935
23.766304	1074.503905	14.805952
23.942517	1074.582784	14.810970
23.593803	1064.516482	14.815987
23.613651	1050.561278	14.821005
23.389214	1051.734335	14.826023
23.136958	1043.642445	14.831040
23.336330	1050.251657	14.836058
23.433753	1069.328603	14.841075
23.627121	1074.016638	14.846093
23.590268	1074.972599	14.851111
23.478365	1066.001054	14.856128
23.638818	1070.371883	14.861146
23.589327	1092.923344	14.866163
23.853712	1092.840303	14.871181
23.635518	1079.656031	14.876199
23.738717	1087.532668	14.881216
24.063280	1083.185194	14.886234
23.741649	1072.482241	14.891251
23.819206	1080.037362	14.896269
23.935566	1069.198495	14.901287
24.107785	1074.105398	14.906304
23.617002	1078.534474	14.911322
23.964713	1085.631254	14.916339
23.934751	1074.921107	14.921357
23.546775	1064.360868	14.926375
23.728388	1074.619022	14.931392
23.724068	1065.454149	14.936410
23.714767	1084.647231	14.941427
24.017678	1105.761459	14.946445
24.385091	1101.370968	14.951463
24.221049	1097.947664	14.956480
24.574373	1096.541742	14.961498
24.271384	1078.400461	14.966515
24.664736	1067.762801	14.971533
24.577878	1060.015739	14.976551
24.479179	1066.537222	14.981568
24.560171	1054.200267	14.986586
24.107315	1073.386999	14.991603
24.410321	1069.875059	14.996621
24.268618	1061.984167	15.001639
24.149240	1064.339057	15.006656
24.225392	1066.678494	15.011674
24.183967	1067.216780	15.016691
24.456767	1061.729314	15.021709
24.156890	1071.925836	15.026727
24.241870	1059.666888	15.031744
24.610414	1065.803982	15.036762
24.202993	1071.237460	15.041779
24.366878	1059.390625	15.046797
24.181705	1072.071416	15.051815
24.218668	1066.461120	15.056832
24.359237	1078.924808	15.061850
24.708540	1092.182590	15.066867
24.792388	1087.758680	15.071885
24.748922	1091.388143	15.076903
24.563401	1098.474021	15.081920
24.923399	1093.079598	15.086938
24.627572	1099.585346	15.091955
24.801362	1087.423890	15.096973
24.810153	1084.100434	15.101991
24.518461	1090.463952	15.107008
24.582949	1094.562243	15.112026
24.679328	1096.860708	15.117043
25.015869	1091.506204	15.122061
25.181581	1094.032701	15.127079
24.942930	1098.374384	15.132096
24.962928	1090.312976	15.137114
24.868871	1093.473904	15.142131
25.057551	1085.682885	15.147149
25.082141	1074.336430	15.152167
24.577267	1059.713030	15.157184
24.931261	1067.087211	15.162202
25.112998	1091.851114	15.167219
25.005140	1088.991406	15.172237
24.892966	1091.445821	15.177255
25.161320	1106.163643	15.182272
25.524222	1090.250415	15.187290
25.096685	1083.311117	15.192307
25.078959	1079.768532	15.197325
25.104908	1092.071195	15.202343
25.057987	1093.590307	15.207360
25.213398	1087.240700	15.212378
25.504748	1096.496700	15.217395
25.131955	1081.285951	15.222413
25.174419	1082.031071	15.227431
25.215126	1085.437906	15.232448
25.756622	1079.261099	15.237466
25.019483	1101.942690	15.242483
24.979406	1095.540890	15.247501
25.041822	1086.865559	15.252519
25.253956	1097.401993	15.257536
25.546802	1092.148836	15.262554
25.401168	1096.334117	15.267571
25.037200	1102.029652	15.272589
25.460773	1098.243658	15.277607
25.435032	1094.603251	15.282624
25.651885	1101.662710	15.287642
25.412948	1089.298100	15.292659
25.371832	1093.038869	15.297677
25.680174	1091.240591	15.302695
25.631034	1085.104497	15.307712
25.761222	1087.592615	15.312730
25.616559	1100.098664	15.317747
25.657331	1091.165673	15.322765
25.874981	1095.794789	15.327783
25.491042	1093.797046	15.332800
25.844699	1102.910986	15.337818
25.800256	1121.485259	15.342835
25.800077	1124.409435	15.347853
26.064789	1125.060913	15.352871
25.685829	1116.743807	15.357888
25.600103	1110.953295	15.362906
25.967640	1122.295484	15.367923
26.312790	1123.489388	15.372941
26.293558	1119.780300	15.377959
25.964413	1109.434005	15.382976
26.051763	1097.258013	15.387994
25.921186	1100.663856	15.393011
26.247021	1111.534509	15.398029
25.977447	1103.967568	15.403047
25.752247	1101.392400	15.408064
26.076201	1110.216940	15.413082
26.175698	1122.482731	15.418099
26.241113	1111.713303	15.423117
26.260274	1112.265522	15.428135
26.148837	1122.170915	15.433152
26.492798	1119.045671	15.438170
26.356275	1121.665989	15.443187
26.256244	1119.187255	15.448205
26.389781	1104.359752	15.453223
26.141705	1109.513013	15.458240
26.420779	1106.767764	15.463258
26.506708	1122.452177	15.468275
26.449739	1123.280795	15.473293
26.646650	1099.349932	15.478311
26.373633	1100.670733	15.483328
26.308596	1081.895349	15.488346
26.289987	1094.379718	15.493363
26.113820	1106.876641	15.498381
26.518237	1105.187303	15.503399
26.248948	1115.550429	15.508416
26.195764	1115.540057	15.513434
26.342225	1120.304798	15.518451
26.649516	1120.101663	15.523469
26.781814	1115.721925	15.528487
26.560781	1123.971174	15.533504
26.741906	1117.836093	15.538522
26.492262	1125.364773	15.543539
26.620908	1119.173570	15.548557
26.541597	1120.800093	15.553575
26.847229	1129.232754	15.558592
26.811912	1143.772539	15.563610
26.825734	1138.949238	15.568627
26.878298	1134.185825	15.573645
27.182085	1140.517316	15.578663
26.700865	1140.233875	15.583680
27.107236	1141.707441	15.588698
27.232056	1141.314765	15.593715
26.873990	1117.249021	15.598733
27.050651	1115.430845	15.603751
26.906296	1136.037600	15.608768
27.044737	1139.488634	15.613786
27.432851	1138.023680	15.618803
27.209594	1132.500474	15.623821
27.173030	1129.344683	15.628839
27.073310	1111.702602	15.633856
26.958213	1114.910933	15.638874
27.334017	1138.217294	15.643891
27.075932	1138.945858	15.648909
27.314537	1130.190495	15.653927
26.921492	1141.984319	15.658944
27.263566	1141.722156	15.663962
27.040448	1145.782962	15.668979
27.093378	1147.809951	15.673997
27.444306	1139.028804	15.679015
27.114904	1148.654385	15.684032
27.289470	1141.442864	15.689050
27.321567	1143.205772	15.694067
27.111268	1137.636455	15.699085
27.404448	1139.230315	15.704103
27.465775	1148.121929	15.709120
27.793035	1144.598238	15.714138
27.498040	1160.851509	15.719155
27.532706	1148.929258	15.724173
27.918907	1139.346568	15.729191
27.734506	1139.832156	15.734208
27.399044	1147.621488	15.739226
27.409375	1145.637934	15.744243
27.850511	1161.772234	15.749261
27.999062	1159.700570	15.754279
27.723038	1157.002942	15.759296
27.512380	1153.201683	15.764314
27.664853	1165.998588	15.769331
28.009924	1170.991210	15.774349
28.165666	1154.351210	15.779367
28.007246	1163.214960	15.784384
27.844884	1165.807947	15.789402
27.701862	1161.135490	15.794419
28.089230	1169.371103	15.799437
28.017384	1163.359715	15.804455
28.215441	1163.403652	15.809472
28.307851	1168.046473	15.814490
28.124445	1141.314978	15.819507
27.925971	1153.329455	15.824525
28.063869	1156.381048	15.829543
28.212556	1156.552404	15.834560
28.338712	1165.153702	15.839578
28.101779	1149.745041	15.844595
28.203184	1164.019233	15.849613
28.126572	1162.779396	15.854631
28.345164	1161.089801	15.859648
28.390803	1160.698742	15.864666
28.461103	1168.237765	15.869683
28.130792	1174.340075	15.874701
28.271180	1166.273582	15.879719
28.112084	1166.368186	15.884736
28.087886	1165.285151	15.889754
28.425689	1158.031858	15.894771
28.285072	1163.180584	15.899789
28.169031	1171.490190	15.904807
28.558415	1168.104445	15.909824
28.482129	1155.353630	15.914842
28.529458	1156.074384	15.919859
28.180310	1172.355179	15.924877
28.698693	1163.265752	15.929895
28.569292	1183.248870	15.934912
28.498012	1198.414192	15.939930
29.156968	1186.900415	15.944947
29.031781	1189.479613	15.949965
29.094086	1178.526594	15.954983
29.125547	1167.789279	15.960000
28.852191	1151.252320	15.965018
28.912565	1150.571059	15.970035
28.766390	1155.569665	15.975053
28.952961	1138.740729	15.980071
28.750218	1162.117375	15.985088
28.267863	1152.526909	15.990106
28.979316	1170.423867	15.995123
28.868584	1174.361369	16.000141
29.112772	1174.289414	16.005159
28.955816	1191.950528	16.010176
29.099574	1194.694467	16.015194
29.406857	1193.289587	16.020211
29.243358	1184.137441	16.025229
29.049548	1157.253426	16.030247
29.049116	1189.941238	16.035264
28.839839	1169.353095	16.040282
28.974256	1194.819970	16.045299
29.192832	1179.690976	16.050317
29.101536	1193.354160	16.055335
29.161167	1188.901049	16.060352
29.125141	1189.825426	16.065370
29.199161	1169.692306	16.070387
29.144068	1211.748008	16.075405
29.332085	1185.383471	16.080423
29.406628	1181.596493	16.085440
29.125278	1180.843892	16.090458
29.345051	1201.851974	16.095475
29.487792	1215.930869	16.100493
30.159548	1207.065484	16.105511
29.792065	1186.238290	16.110528
29.849223	1183.084843	16.115546
29.915288	1179.901662	16.120563
29.636651	1186.053936	16.125581
30.084173	1174.161772	16.130599
29.921026	1171.820505	16.135616
29.557459	1198.924037	16.140634
29.926807	1158.572148	16.145651
29.762832	1181.969383	16.150669
29.537542	1169.726791	16.155687
29.741799	1186.089225	16.160704
29.648860	1170.412195	16.165722
29.947823	1175.492393	16.170739
29.729295	1175.041221	16.175757
29.627075	1180.770543	16.180775
29.892807	1183.561092	16.185792
29.768688	1209.006305	16.190810
30.367643	1213.735091	16.195827
30.691480	1198.269979	16.200845
30.506600	1176.215078	16.205863
30.129170	1190.045010	16.210880
30.068543	1174.376980	16.215898
30.179333	1164.640003	16.220915
30.203699	1162.204341	16.225933
29.963657	1183.329771	16.230951
30.234327	1172.519699	16.235968
30.024543	1174.731729	16.240986
30.031307	1201.414424	16.246003
30.211925	1183.814060	16.251021
30.520414	1211.189520	16.256039
30.295213	1186.569235	16.261056
30.563133	1208.082435	16.266074
30.804329	1181.943794	16.271091
30.558985	1193.964206	16.276109
30.669533	1201.732772	16.281127
30.501632	1179.661002	16.286144
30.517826	1167.570228	16.291162
30.831559	1175.984323	16.296179
30.742399	1174.167636	16.301197
30.504730	1185.576507	16.306215
30.331393	1174.189183	16.311232
30.454947	1185.512133	16.316250
30.709881	1193.647763	16.321267
30.642216	1203.333881	16.326285
30.654686	1201.782543	16.331303
31.120224	1187.082900	16.336320
30.763209	1199.358643	16.341338
30.849798	1206.703186	16.346355
31.049886	1188.984884	16.351373
31.132630	1200.930957	16.356391
31.118213	1208.288463	16.361408
30.993059	1192.451385	16.366426
31.024965	1205.523947	16.371443
31.211120	1196.674666	16.376461
31.087623	1183.223522	16.381479
31.143359	1190.794765	16.386496
30.756586	1208.983315	16.391514
31.104785	1195.782537	16.396531
31.045325	1196.710652	16.401549
31.059004	1194.551958	16.406567
30.890175	1211.835905	16.411584
31.008423	1198.144854	16.416602
31.347844	1195.797362	16.421619
31.185241	1204.871009	16.426637
30.945479	1190.068347	16.431655
31.049072	1192.460056	16.436672
31.245290	1211.211559	16.441690
31.558338	1214.546680	16.446707
31.438687	1227.097612	16.451725
31.773999	1221.183281	16.456743
31.606442	1214.501321	16.461760
31.639948	1204.337786	16.466778
31.507813	1192.956459	16.471795
31.565205	1191.898161	16.476813
31.564090	1207.258361	16.481831
31.704158	1205.804646	16.486848
31.593128	1208.965160	16.491866
31.991423	1221.475955	16.496883
31.858685	1231.818960	16.501901
31.514968	1197.010570	16.506919
31.859097	1193.650912	16.511936
31.858508	1218.008398	16.516954
31.945310	1226.255800	16.521971
32.086126	1208.977919	16.526989
31.995147	1189.103884	16.532007
31.995097	1196.728070	16.537024
31.661816	1195.076149	16.542042
32.092587	1197.555674	16.547059
32.146679	1207.618765	16.552077
32.132472	1203.639876	16.557095
32.226012	1193.108138	16.562112
31.933357	1194.784423	16.567130
32.202409	1192.551970	16.572147
32.301419	1184.750032	16.577165
32.130731	1202.400765	16.582183
32.242160	1190.472529	16.587200
32.058434	1191.151485	16.592218
32.409698	1216.159115	16.597235
32.593327	1223.382802	16.602253
32.392640	1198.340178	16.607271
32.400290	1191.850502	16.612288
32.352866	1206.370259	16.617306
32.673649	1197.988699	16.622323
32.457803	1188.568056	16.627341
32.059123	1185.617861	16.632359
32.661925	1217.588213	16.637376
32.472273	1212.551955	16.642394
32.142606	1223.785199	16.647411
32.694445	1219.119879	16.652429
32.492849	1211.370586	16.657447
32.450078	1231.081988	16.662464
32.417350	1218.438997	16.667482
32.548510	1203.548853	16.672499
32.900911	1213.370899	16.677517
32.656205	1219.520921	16.682535
32.714441	1201.268396	16.687552
32.685246	1240.811175	16.692570
33.007571	1195.815411	16.697587
32.584252	1233.865364	16.702605
32.755108	1202.904172	16.707623
33.033200	1216.359037	16.712640
33.031961	1279.650851	16.717658
32.622398	1247.890252	16.722675
33.335125	1208.801610	16.727693
33.543262	1269.488190	16.732711
33.075840	1260.504011	16.737728
33.400911	1227.265678	16.742746
33.148856	1264.135411	16.747763
33.236591	1264.849727	16.752781
32.962708	1234.406118	16.757799
33.717274	1206.607874	16.762816
33.255534	1220.844522	16.767834
33.135710	1258.141448	16.772851
33.317836	1266.419287	16.777869
32.909953	1240.679774	16.782887
33.480858	1224.270775	16.787904
33.381167	1255.546311	16.792922
33.080857	1234.538453	16.797939
33.710649	1220.726475	16.802957
33.428984	1222.883911	16.807975
33.532256	1262.493710	16.812992
33.335199	1223.378666	16.818010
33.084946	1270.986782	16.823027
33.500596	1257.208921	16.828045
33.268209	1255.709210	16.833063
33.870508	1245.602795	16.838080
33.691923	1277.663289	16.843098
34.508933	1236.058488	16.848115
34.109117	1264.201364	16.853133
33.996888	1227.551784	16.858151
33.841270	1243.177327	16.863168
33.753491	1230.695683	16.868186
33.643723	1229.492586	16.873203
34.029744	1249.591791	16.878221
34.000178	1259.089406	16.883239
34.359325	1256.247993	16.888256
34.080798	1240.182074	16.893274
34.317813	1259.564187	16.898291
34.287321	1237.410642	16.903309
33.793103	1237.192189	16.908327
34.271555	1261.706151	16.913344
34.595320	1241.467036	16.918362
34.113242	1236.321681	16.923379
34.332213	1259.782235	16.928397
34.414945	1258.282605	16.933415
34.497083	1249.114838	16.938432
34.053486	1241.979829	16.943450
34.447161	1262.725895	16.948467
34.159234	1258.454028	16.953485
34.282590	1256.616022	16.958503
34.488412	1263.271494	16.963520
34.515019	1259.890102	16.968538
34.026263	1261.188695	16.973555
34.491552	1262.799166	16.978573
34.453856	1256.456687	16.983591
34.708917	1252.170583	16.988608
34.721940	1276.716327	16.993626
34.724656	1267.907268	16.998643
35.134065	1262.369628	17.003661
34.536743	1261.661121	17.008679
34.734973	1256.559843	17.013696
34.716376	1267.801712	17.018714
34.781342	1261.390950	17.023731
35.022981	1270.096587	17.028749
34.814136	1272.099276	17.033767
35.082565	1287.959251	17.038784
34.932235	1296.795052	17.043802
35.161407	1275.419558	17.048819
35.208851	1313.921590	17.053837
34.705221	1294.904426	17.058855
35.147100	1300.156926	17.063872
35.335797	1285.016858	17.068890
34.931595	1312.455834	17.073907
35.239262	1284.779047	17.078925
35.360375	1297.359281	17.083943
35.785425	1288.937447	17.088960
35.557293	1287.106730	17.093978
35.671053	1285.119245	17.098995
35.617421	1282.110856	17.104013
35.235997	1281.155565	17.109031
35.741378	1262.427399	17.114048
35.558277	1265.824353	17.119066
35.262844	1269.248661	17.124083
35.816476	1259.437852	17.129101
35.440363	1265.127520	17.134119
35.669749	1283.829786	17.139136
35.387324	1266.320470	17.144154
35.709578	1299.793890	17.149171
36.209450	1260.032790	17.154189
35.811625	1304.738825	17.159207
35.759907	1269.447978	17.164224
36.041858	1292.980337	17.169242
35.862169	1283.860596	17.174259
36.453270	1251.562890	17.179277
35.896353	1270.426715	17.184295
35.973273	1243.456891	17.189312
35.612483	1240.620187	17.194330
36.269895	1262.105958	17.199347
36.166365	1257.570311	17.204365
35.670654	1264.501251	17.209383
35.988342	1276.735524	17.214400
36.061751	1279.570920	17.219418
36.126516	1275.914461	17.224435
36.213305	1269.493924	17.229453
35.906785	1292.163762	17.234471
36.157592	1275.963051	17.239488
35.995784	1265.459399	17.244506
36.067048	1260.526227	17.249523
36.031614	1280.139001	17.254541
36.485543	1287.953523	17.259559
36.440105	1299.462384	17.264576
36.694138	1299.187519	17.269594
36.493485	1316.932830	17.274611
36.620123	1292.984541	17.279629
36.365779	1318.623741	17.284647
36.438242	1287.388632	17.289664
36.469890	1297.181667	17.294682
36.330184	1322.972474	17.299699
36.737259	1298.941701	17.304717
36.824571	1303.972331	17.309735
36.883991	1301.070174	17.314752
37.115204	1305.989770	17.319770
36.528189	1295.772550	17.324787
36.867890	1316.281917	17.329805
36.860978	1291.455186	17.334823
37.104333	1302.463404	17.339840
36.625901	1310.141919	17.344858
36.890339	1292.878829	17.349875
36.870381	1311.079792	17.354893
36.875457	1288.901619	17.359911
37.249889	1340.040765	17.364928
37.037670	1314.095315	17.369946
37.070917	1339.830256	17.374963
37.317384	1322.862571	17.379981
37.301345	1338.797855	17.384999
37.455363	1332.132195	17.390016
37.343487	1323.100711	17.395034
37.257745	1328.341414	17.400051
37.641044	1334.216731	17.405069
37.886764	1331.849557	17.410087
37.593642	1323.194606	17.415104
37.991341	1330.516339	17.420122
37.646833	1303.000151	17.425139
37.637157	1300.725619	17.430157
37.407988	1296.787279	17.435175
37.482889	1303.484097	17.440192
37.538424	1307.692411	17.445210
37.357896	1307.184837	17.450227
37.905244	1331.395358	17.455245
37.622058	1304.012530	17.460263
37.745022	1345.624174	17.465280
37.833044	1326.318350	17.470298
37.965163	1330.797594	17.475315
37.682560	1333.137660	17.480333
37.779698	1319.610305	17.485351
37.685701	1318.992980	17.490368
38.017418	1334.465399	17.495386
38.025359	1317.740246	17.500403
38.054804	1319.852800	17.505421
38.063001	1338.244356	17.510439
38.059394	1330.446120	17.515456
38.281292	1331.118595	17.520474
38.148798	1361.895452	17.525491
38.380936	1350.726461	17.530509
38.147546	1360.527200	17.535527
38.697069	1343.494644	17.540544
38.817972	1339.258224	17.545562
38.214700	1359.781972	17.550579
38.541684	1335.904692	17.555597
38.067378	1348.343193	17.560615
38.448126	1355.639328	17.565632
38.592645	1336.433016	17.570650
38.764069	1345.023271	17.575667
38.867121	1340.899019	17.580685
38.650402	1353.598458	17.585703
38.926811	1331.670309	17.590720
38.553507	1350.230470	17.595738
38.415993	1343.314790	17.600755
38.554649	1374.617851	17.605773
38.736721	1375.644309	17.610791
38.803522	1377.474068	17.615808
38.940781	1375.390018	17.620826
38.709854	1376.560989	17.625843
38.904734	1371.648963	17.630861
38.802906	1373.101357	17.635879
38.463176	1361.605144	17.640896
38.852140	1367.473279	17.645914
39.091536	1368.569243	17.650931
39.411039	1360.928670	17.655949
39.478701	1354.108462	17.660967
39.433537	1389.687135	17.665984
39.559602	1371.508520	17.671002
39.734599	1348.975976	17.676019
39.655750	1382.947700	17.681037
39.170038	1342.877161	17.686055
39.840065	1328.136900	17.691072
39.818552	1348.693694	17.696090
39.946816	1338.202716	17.701107
39.317811	1326.699181	17.706125
39.976682	1297.031598	17.711143
39.529862	1327.807389	17.716160
39.842246	1335.850571	17.721178
39.837302	1308.041127	17.726195
39.510133	1341.171488	17.731213
39.879762	1332.264551	17.736231
39.514842	1316.080194	17.741248
39.764395	1338.518283	17.746266
39.598789	1327.640822	17.751283
39.365575	1360.432995	17.756301
39.945295	1341.729837	17.761319
39.744018	1381.225727	17.766336
39.970602	1344.196210	17.771354
39.935582	1382.768204	17.776371
39.921833	1353.607311	17.781389
40.038645	1344.553501	17.786407
40.029418	1389.344111	17.791424
39.743526	1362.381591	17.796442
39.908880	1352.012887	17.801459
40.227507	1389.775043	17.806477
40.273100	1385.786568	17.811495
40.201378	1406.511109	17.816512
40.507762	1385.694134	17.821530
40.011082	1394.067716	17.826547
40.328613	1394.314393	17.831565
40.629077	1387.365810	17.836583
40.307775	1393.238691	17.841600
40.844554	1385.734910	17.846618
40.344995	1385.001366	17.851635
40.810167	1389.271789	17.856653
40.655912	1383.230979	17.861671
40.360115	1409.227726	17.866688
40.803126	1394.429223	17.871706
40.536767	1400.309074	17.876723
40.755219	1400.087072	17.881741
41.020951	1424.949834	17.886759
41.009655	1422.680261	17.891776
41.521266	1410.461514	17.896794
41.248206	1400.780875	17.901811
41.175705	1381.057782	17.906829
41.043816	1386.428558	17.911847
40.976817	1380.406867	17.916864
41.220777	1379.491831	17.921882
40.879737	1388.334506	17.926899
41.056300	1385.470278	17.931917
40.987294	1408.199944	17.936935
41.105412	1421.653772	17.941952
41.139896	1400.216336	17.946970
40.628757	1421.923308	17.951987
41.109159	1410.466146	17.957005
41.213126	1429.445000	17.962023
41.054093	1415.952115	17.967040
41.655734	1449.747835	17.972058
41.673263	1436.859117	17.977075
41.388485	1442.483952	17.982093
41.629867	1451.597144	17.987111
41.841265	1435.131986	17.992128
42.162218	1432.648981	17.997146
42.139691	1443.723303	18.002163
41.898768	1425.749433	18.007181
42.195314	1444.331088	18.012199
42.166840	1415.442974	18.017216
42.240547	1399.466992	18.022234
41.551690	1411.294050	18.027251
41.800357	1409.369976	18.032269
42.209910	1418.338354	18.037287
42.192245	1439.186453	18.042304
42.515144	1417.839845	18.047322
42.104624	1415.640231	18.052339
42.153872	1408.563391	18.057357
42.410959	1408.575895	18.062375
42.169553	1410.923561	18.067392
42.238910	1430.920940	18.072410
42.103648	1441.401346	18.077427
42.141227	1423.845524	18.082445
42.430441	1441.294219	18.087463
41.706212	1435.702927	18.092480
42.564948	1405.635170	18.097498
42.445890	1454.003166	18.102515
42.450137	1434.303939	18.107533
42.793995	1436.298731	18.112551
42.420964	1443.408386	18.117568
42.840153	1440.228608	18.122586
42.747765	1446.963182	18.127603
42.705781	1470.376034	18.132621
43.065394	1446.050572	18.137639
42.795807	1473.954439	18.142656
43.194515	1457.733085	18.147674
43.071605	1443.373987	18.152691
42.856268	1472.334115	18.157709
43.296070	1441.598506	18.162727
43.006303	1479.262868	18.167744
43.495859	1445.378045	18.172762
42.921411	1445.460239	18.177779
43.338295	1444.550654	18.182797
43.595086	1435.219640	18.187815
42.856893	1433.636982	18.192832
43.081712	1453.158151	18.197850
43.457187	1431.735500	18.202867
43.218815	1467.437983	18.207885
43.361607	1442.285104	18.212903
43.348196	1465.257672	18.217920
43.693755	1448.761665	18.222938
43.673172	1447.094452	18.227955
43.918380	1458.988089	18.232973
43.962410	1440.229452	18.237991
43.776313	1453.044427	18.243008
43.709499	1443.066605	18.248026
44.025464	1443.252187	18.253043
43.760792	1455.134327	18.258061
43.849025	1444.085739	18.263079
43.969420	1440.626429	18.268096
44.186725	1436.030123	18.273114
43.778593	1460.811652	18.278131
43.872398	1446.218220	18.283149
44.132526	1450.198898	18.288167
43.683195	1462.719241	18.293184
43.922104	1449.875429	18.298202
44.184926	1438.754958	18.303219
43.918877	1449.050165	18.308237
44.335926	1447.896741	18.313255
44.213052	1444.501393	18.318272
44.090839	1437.654798	18.323290
44.071018	1466.665531	18.328307
44.661892	1476.394673	18.333325
44.777281	1468.276944	18.338343
44.519293	1460.236067	18.343360
44.666335	1472.722659	18.348378
44.532572	1458.889083	18.353395
44.460732	1463.872793	18.358413
44.690538	1490.534610	18.363431
44.896407	1470.210161	18.368448
44.861662	1471.634564	18.373466
44.979649	1469.377399	18.378483
45.127483	1478.216097	18.383501
45.288651	1463.179332	18.388519
45.053945	1456.591336	18.393536
44.585251	1436.003284	18.398554
44.758434	1456.632213	18.403571
44.735141	1468.865973	18.408589
45.080166	1461.754522	18.413607
44.586411	1474.241061	18.418624
44.724661	1462.094398	18.423642
44.944210	1467.566457	18.428659
44.957235	1481.093729	18.433677
45.453115	1478.041710	18.438695
45.192091	1495.411481	18.443712
45.419344	1486.764679	18.448730
45.331593	1497.489228	18.453747
45.295012	1498.023611	18.458765
45.530155	1487.217398	18.463783
45.340478	1500.556794	18.468800
45.746529	1492.809543	18.473818
45.700606	1491.582086	18.478835
45.470833	1494.659352	18.483853
45.724017	1490.799762	18.488871
45.774150	1494.628327	18.493888
45.769990	1492.563667	18.498906
45.820849	1492.843437	18.503923
45.641629	1492.787097	18.508941
45.581187	1491.517911	18.513959
45.452612	1501.655954	18.518976
45.853513	1515.181175	18.523994
45.855354	1510.147307	18.529011
45.721209	1540.966492	18.534029
46.284856	1516.049959	18.539047
46.256944	1521.813183	18.544064
46.296877	1531.301466	18.549082
46.527516	1506.507268	18.554099
46.662172	1512.052657	18.559117
46.595982	1518.268715	18.564135
46.596608	1515.075449	18.569152
46.790216	1501.088954	18.574170
46.653256	1520.255783	18.579187
46.556732	1514.888393	18.584205
47.056586	1503.374576	18.589223
46.917864	1515.416001	18.594240
46.561042	1513.866894	18.599258
47.326252	1509.238244	18.604275
46.653469	1507.689189	18.609293
46.703512	1503.083356	18.614311
46.586513	1496.904426	18.619328
46.820908	1506.824143	18.624346
47.103481	1513.536703	18.629363
47.317814	1517.123588	18.634381
47.050663	1509.489979	18.639399
46.910781	1506.149237	18.644416
46.786160	1513.966486	18.649434
47.334180	1500.489752	18.654451
46.953493	1506.936854	18.659469
47.154790	1503.338788	18.664487
47.072839	1502.826497	18.669504
47.114623	1499.714758	18.674522
47.319296	1509.368661	18.679539
46.959747	1526.640926	18.684557
47.672950	1523.678508	18.689575
47.499063	1524.107374	18.694592
47.461793	1531.806885	18.699610
47.555599	1527.010025	18.704627
47.497871	1541.218734	18.709645
47.708780	1530.405343	18.714663
47.863377	1529.001189	18.719680
47.684814	1525.496727	18.724698
47.982979	1541.644819	18.729715
47.598744	1519.183890	18.734733
47.685675	1526.028328	18.739751
47.824248	1545.229900	18.744768
47.680202	1533.504143	18.749786
47.898681	1541.829826	18.754803
47.908522	1549.161616	18.759821
48.428888	1555.553134	18.764839
48.329529	1561.824837	18.769856
48.485906	1561.398804	18.774874
48.757188	1528.902952	18.779891
48.165586	1535.349095	18.784909
48.672552	1522.865160	18.789927
48.393484	1530.834461	18.794944
48.132835	1534.160475	18.799962
48.193361	1528.365347	18.804979
48.370913	1547.279139	18.809997
48.748750	1556.582993	18.815015
48.835898	1561.876432	18.820032
48.836661	1552.353367	18.825050
48.961714	1546.739848	18.830067
48.877108	1557.594500	18.835085
49.068369	1545.944246	18.840103
49.039962	1552.457884	18.845120
48.594709	1544.081886	18.850138
48.983067	1555.811205	18.855155
48.844574	1556.484536	18.860173
48.884589	1551.156706	18.865191
48.851894	1554.370867	18.870208
48.942103	1563.596328	18.875226
49.050708	1560.867171	18.880243
48.827771	1553.577266	18.885261
49.007877	1550.257843	18.890279
49.360362	1583.285088	18.895296
49.347257	1556.818243	18.900314
49.740345	1588.321076	18.905331
49.977321	1567.403226	18.910349
49.942427	1566.603434	18.915367
49.601435	1567.993315	18.920384
49.407033	1570.116435	18.925402
49.706337	1557.608958	18.930419
49.460018	1568.604235	18.935437
49.461075	1570.880227	18.940455
49.807409	1576.497275	18.945472
49.650415	1573.365310	18.950490
49.739064	1566.588846	18.955507
49.625339	1577.484335	18.960525
49.624835	1572.329698	18.965543
50.131874	1578.109880	18.970560
50.158027	1582.764975	18.975578
50.567421	1598.137203	18.980595
50.426404	1573.246431	18.985613
50.207811	1566.718735	18.990631
50.152900	1585.227633	18.995648
50.164488	1561.751847	19.000666
50.274871	1601.631998	19.005683
50.060925	1581.940625	19.010701
50.412280	1603.216170	19.015719
50.622194	1595.141498	19.020736
50.144940	1609.532006	19.025754
50.775358	1580.201863	19.030771
50.425107	1611.533855	19.035789
50.921090	1591.214881	19.040807
50.945964	1583.117816	19.045824
50.575462	1596.155804	19.050842
50.588996	1602.790189	19.055859
50.404011	1595.541401	19.060877
51.001079	1597.152921	19.065895
51.079049	1604.110509	19.070912
50.888840	1630.487211	19.075930
51.342434	1615.625449	19.080947
51.205232	1627.806723	19.085965
51.081543	1635.430408	19.090983
51.510145	1627.825780	19.096000
51.363961	1629.127972	19.101018
51.225291	1622.718065	19.106035
51.213285	1637.438670	19.111053
51.501460	1625.883009	19.116071
51.496457	1614.076812	19.121088
51.439217	1628.768443	19.126106
51.880555	1619.011483	19.131123
51.696215	1614.454003	19.136141
51.802149	1619.447169	19.141159
52.180742	1612.929609	19.146176
51.630438	1632.692607	19.151194
51.925830	1626.120670	19.156211
51.927376	1603.167085	19.161229
51.597881	1636.106581	19.166247
52.107244	1601.644086	19.171264
51.561942	1623.624216	19.176282
51.873072	1617.694708	19.181299
51.825029	1628.246282	19.186317
51.790107	1612.795471	19.191335
52.072413	1649.315129	19.196352
52.443863	1631.581545	19.201370
52.402980	1650.874796	19.206387
52.447640	1644.632270	19.211405
52.925007	1639.063204	19.216423
53.034329	1638.924670	19.221440
52.541960	1644.367184	19.226458
52.272578	1603.365590	19.231475
52.760810	1646.226234	19.236493
52.841844	1622.830509	19.241511
52.993204	1652.053412	19.246528
53.053045	1616.688872	19.251546
52.386586	1622.654638	19.256563
52.817080	1626.883474	19.261581
52.703998	1631.902133	19.266599
52.770102	1627.454147	19.271616
52.587713	1646.876923	19.276634
52.944035	1628.801264	19.281651
52.754911	1636.388195	19.286669
52.825602	1633.561251	19.291687
53.039858	1637.280312	19.296704
53.118579	1647.998874	19.301722
53.374500	1648.585716	19.306739
53.342394	1655.804700	19.311757
53.230953	1660.785354	19.316775
53.791304	1667.846944	19.321792
53.601491	1669.130928	19.326810
53.548594	1661.323072	19.331827
53.896845	1660.378804	19.336845
53.721035	1661.259436	19.341863
53.682369	1655.152889	19.346880
53.325122	1664.015617	19.351898
53.681721	1658.992764	19.356915
53.827000	1671.717334	19.361933
53.608555	1652.712417	19.366951
53.842461	1648.700131	19.371968
53.662527	1661.951605	19.376986
53.781449	1679.103704	19.382003
54.098566	1682.479187	19.387021
53.869297	1690.892089	19.392039
54.091549	1683.723032	19.397056
54.313379	1689.437058	19.402074
54.484293	1686.587830	19.407091
54.397192	1680.402480	19.412109
54.058425	1683.300540	19.417127
54.237930	1677.228404	19.422144
54.254165	1683.445546	19.427162
54.713326	1694.451110	19.432179
54.927779	1689.304624	19.437197
54.762998	1712.655652	19.442215
54.852156	1680.624231	19.447232
54.584413	1686.108017	19.452250
54.719308	1705.997798	19.457267
55.159123	1686.320003	19.462285
55.184058	1695.272814	19.467303
55.426038	1712.090724	19.472320
55.376079	1688.810163	19.477338
55.278916	1694.195964	19.482355
55.454178	1674.964638	19.487373
55.232801	1659.172279	19.492391
55.171168	1680.516944	19.497408
55.492056	1642.674108	19.502426
55.377665	1680.284284	19.507443
55.584875	1657.952189	19.512461
55.285922	1696.027563	19.517479
55.963315	1680.047811	19.522496
55.405793	1705.825704	19.527514
55.824302	1690.271041	19.532531
55.812986	1689.253551	19.537549
55.830024	1697.927626	19.542567
55.978643	1692.127822	19.547584
55.658483	1691.316886	19.552602
55.789939	1699.275868	19.557619
55.837270	1701.233042	19.562637
55.776203	1692.333223	19.567655
56.092382	1679.994410	19.572672
55.915414	1702.216366	19.577690
56.449189	1677.320053	19.582707
56.129500	1708.853446	19.587725
55.821431	1686.048203	19.592743
56.200464	1704.595019	19.597760
56.517296	1692.492043	19.602778
56.423529	1685.382819	19.607795
56.116988	1698.220363	19.612813
56.132603	1701.702132	19.617831
56.497345	1696.597743	19.622848
56.431348	1723.329184	19.627866
56.404380	1722.762499	19.632883
56.846334	1721.892948	19.637901
56.668362	1717.472846	19.642919
56.884468	1715.948754	19.647936
56.812716	1739.156003	19.652954
57.064506	1712.953370	19.657971
57.048031	1723.426047	19.662989
56.989257	1724.520827	19.668007
57.164595	1718.645966	19.673024
56.999062	1733.337669	19.678042
56.759834	1724.996350	19.683059
57.198310	1755.111196	19.688077
57.124678	1745.658071	19.693095
57.361310	1748.544609	19.698112
57.544804	1764.599553	19.703130
57.467797	1740.667269	19.708147
57.611824	1732.032021	19.713165
57.563493	1754.036916	19.718183
57.717894	1739.479144	19.723200
57.631568	1729.666257	19.728218
57.431515	1755.027010	19.733235
58.011901	1746.454302	19.738253
57.975274	1761.746822	19.743271
58.173454	1783.714023	19.748288
58.139797	1776.138991	19.753306
58.134215	1773.780361	19.758323
58.148352	1783.175396	19.763341
57.945413	1752.909715	19.768359
58.446400	1789.948561	19.773376
58.533345	1744.131333	19.778394
58.328201	1782.100738	19.783411
58.649437	1757.211440	19.788429
58.611213	1776.147357	19.793447
58.754441	1749.132985	19.798464
58.724780	1771.012232	19.803482
58.648625	1755.583574	19.808499
58.949682	1774.737518	19.813517
59.088376	1753.369458	19.818535
58.701897	1762.417805	19.823552
58.877477	1724.344670	19.828570
58.501962	1784.127618	19.833587
58.719314	1762.353743	19.838605
58.954268	1773.911076	19.843623
58.853015	1746.304913	19.848640
59.078042	1774.127335	19.853658
59.211836	1765.081566	19.858675
59.220955	1737.998939	19.863693
59.017080	1777.718904	19.868711
59.299556	1744.212475	19.873728
59.191757	1763.258571	19.878746
59.395755	1759.271474	19.883763
59.445235	1775.116566	19.888781
59.524926	1805.188058	19.893799
59.820281	1775.434328	19.898816
59.572316	1798.690221	19.903834
59.636308	1793.773759	19.908851
59.859180	1785.679612	19.913869
59.899976	1793.867036	19.918887
60.184336	1770.978196	19.923904
59.806559	1797.449607	19.928922
59.756755	1787.399621	19.933939
59.906033	1774.484873	19.938957
59.758961	1793.035475	19.943975
60.028882	1774.880605	19.948992
59.895865	1786.830110	19.954010
60.124303	1815.608469	19.959027
60.357084	1813.318788	19.964045
60.298296	1798.513382	19.969063
60.384538	1832.129495	19.974080
60.584395	1805.032056	19.979098
60.558875	1823.085111	19.984115
60.662638	1799.542330	19.989133
60.264986	1818.165957	19.994151
60.753125	1822.033301	19.999168
60.631391	1810.763086	20.004186
60.374387	1852.610601	20.009203
60.715042	1822.796067	20.014221
60.671945	1834.419811	20.019239
60.979418	1816.921147	20.024256
61.348841	1839.031013	20.029274
61.048809	1832.192137	20.034291
61.150260	1812.152851	20.039309
61.278179	1864.665523	20.044327
61.457854	1847.330349	20.049344
61.740253	1837.213197	20.054362
61.743164	1866.068520	20.059379
62.005492	1815.340392	20.064397
61.815178	1839.405134	20.069415
61.928448	1828.399452	20.074432
61.827028	1812.062404	20.079450
61.752024	1824.274822	20.084467
61.955220	1811.713241	20.089485
62.009356	1814.383502	20.094503
62.166431	1804.353997	20.099520
62.226850	1818.320767	20.104538
61.633909	1814.459168	20.109555
61.902243	1797.489016	20.114573
62.187930	1832.596018	20.119591
62.304267	1836.535241	20.124608
62.593552	1817.211612	20.129626
62.220919	1846.899143	20.134643
62.402958	1834.556421	20.139661
62.490500	1831.918663	20.144679
62.318176	1842.194481	20.149696
62.469253	1841.253331	20.154714
62.163173	1837.451374	20.159731
62.749345	1817.695008	20.164749
62.868988	1858.258659	20.169767
62.775452	1825.077848	20.174784
62.481706	1845.445163	20.179802
62.686623	1840.073628	20.184819
62.946663	1845.468589	20.189837
62.826437	1873.544462	20.194855
63.127782	1843.297277	20.199872
63.419577	1876.501613	20.204890
63.489611	1837.941640	20.209907
63.204954	1870.250021	20.214925
63.386828	1845.914482	20.219943
62.994636	1863.599767	20.224960
63.718927	1858.666077	20.229978
63.177632	1864.706361	20.234995
63.517761	1861.413261	20.240013
63.362260	1864.565276	20.245031
63.709605	1872.381388	20.250048
64.056577	1875.865415	20.255066
63.625856	1905.394012	20.260083
64.276425	1861.547219	20.265101
64.150635	1857.642573	20.270119
64.017997	1910.645278	20.275136
63.791025	1873.917975	20.280154
64.174190	1891.138301	20.285171
64.022660	1878.475925	20.290189
64.219379	1880.631100	20.295207
63.947752	1894.419656	20.300224
64.577444	1880.983034	20.305242
64.541126	1912.948312	20.310259
64.898033	1905.056098	20.315277
65.047833	1915.850041	20.320295
64.483488	1872.314931	20.325312
64.824944	1901.301956	20.330330
64.791715	1890.626332	20.335347
65.280331	1892.572939	20.340365
65.144057	1897.203699	20.345383
65.378768	1900.573499	20.350400
64.879667	1865.940856	20.355418
64.661327	1889.604306	20.360435
65.096069	1896.031657	20.365453
65.532194	1888.118954	20.370471
65.121028	1912.502182	20.375488
65.463241	1871.771963	20.380506
65.169622	1920.101710	20.385523
65.099932	1889.973371	20.390541
65.142327	1909.211214	20.395559
64.965417	1905.613585	20.400576
65.730852	1906.930879	20.405594
65.557026	1940.292983	20.410611
66.025976	1921.834055	20.415629
65.903870	1919.692187	20.420647
65.804933	1943.671743	20.425664
66.122874	1915.229191	20.430682
66.069628	1929.983412	20.435699
66.406015	1928.696525	20.440717
66.302754	1918.818569	20.445735
66.121542	1926.634052	20.450752
66.565335	1907.109485	20.455770
66.456625	1932.427666	20.460787
66.379112	1920.272555	20.465805
66.788419	1924.835200	20.470823
66.087888	1941.909070	20.475840
66.411843	1901.905279	20.480858
66.178278	1929.041351	20.485875
65.894402	1936.892087	20.490893
66.554027	1916.077800	20.495911
66.688383	1966.194071	20.500928
66.735412	1950.246906	20.505946
66.780338	1942.383972	20.510963
67.013229	1920.352550	20.515981
67.221450	1932.027532	20.520999
66.961781	1991.364990	20.526016
67.148379	1973.349004	20.531034
67.702880	1961.201615	20.536051
67.630557	1984.042826	20.541069
67.724291	1964.680971	20.546087
67.321358	1993.723963	20.551104
68.319937	1961.425777	20.556122
67.749973	1966.791117	20.561139
67.398423	1975.535145	20.566157
67.898965	1945.955989	20.571175
67.598655	1997.069777	20.576192
67.447796	1973.587767	20.581210
67.963203	1950.875736	20.586227
67.938208	1979.155280	20.591245
68.010798	2007.749659	20.596263
67.656437	1981.564549	20.601280
68.256180	1953.528450	20.606298
68.153101	2008.274453	20.611315
67.874411	1997.239910	20.616333
68.612571	1978.681352	20.621351
68.586120	1988.347264	20.626368
68.519547	2011.047599	20.631386
68.292916	2001.955337	20.636403
68.503710	1985.242684	20.641421
69.024029	1966.116401	20.646439
68.676159	2015.812658	20.651456
68.886905	1980.805418	20.656474
68.910942	2002.144759	20.661491
68.949108	2025.342803	20.666509
69.441858	1997.781440	20.671527
69.274952	2032.898178	20.676544
69.721127	2018.353377	20.681562
68.953010	2001.877032	20.686579
69.424533	1980.762308	20.691597
69.464318	2033.347849	20.696615
69.382883	2006.315341	20.701632
69.636654	2013.882179	20.706650
69.555660	2003.325775	20.711667
69.633451	2031.389253	20.716685
69.549385	1996.097073	20.721703
69.646883	2023.691770	20.726720
69.649061	2005.900211	20.731738
69.478166	2013.997245	20.736755
69.870557	2027.061830	20.741773
70.261501	2028.849422	20.746791
69.943908	2027.769062	20.751808
70.437218	2060.594041	20.756826
70.055015	2037.397362	20.761843
70.258772	2037.473432	20.766861
70.498998	2034.952865	20.771879
70.375383	2046.111409	20.776896
70.270637	2043.375284	20.781914
70.722302	2013.168271	20.786931
70.648290	2010.400510	20.791949
70.479318	2053.543346	20.796967
70.327759	2056.834776	20.801984
70.983060	2060.974412	20.807002
71.346572	2056.571680	20.812019
71.229981	2080.354498	20.817037
71.324885	2072.694314	20.822055
71.186611	2072.997963	20.827072
71.566004	2048.209009	20.832090
71.459150	2073.157471	20.837107
71.819786	2038.826201	20.842125
72.086062	2071.539542	20.847143
71.485016	2057.845975	20.852160
71.948027	2050.866441	20.857178
71.817875	2058.456770	20.862195
71.884724	2045.545488	20.867213
72.161936	2051.892635	20.872231
71.751795	2036.729298	20.877248
71.699877	2055.592257	20.882266
71.797492	2063.418407	20.887283
71.836855	2041.944637	20.892301
72.026035	2070.234251	20.897319
71.864284	2060.798117	20.902336
72.072804	2040.192445	20.907354
71.853508	2079.981764	20.912371
71.847366	2061.326281	20.917389
72.317767	2089.687495	20.922407
72.323285	2070.509457	20.927424
72.362786	2079.441305	20.932442
72.242334	2093.152458	20.937459
72.712310	2086.645288	20.942477
73.125276	2089.368494	20.947495
72.907476	2123.216241	20.952512
72.869525	2098.872860	20.957530
72.868447	2119.079055	20.962547
73.135227	2119.192268	20.967565
73.154290	2089.288468	20.972583
73.022492	2125.088832	20.977600
73.238610	2086.849404	20.982618
73.123890	2120.042044	20.987635
73.410022	2085.936480	20.992653
73.446381	2111.875223	20.997671
73.405365	2084.828258	21.002688
73.637023	2125.912782	21.007706
73.832695	2132.125099	21.012723
73.864580	2140.350320	21.017741
74.183624	2128.633606	21.022759
73.923898	2134.157179	21.027776
74.057261	2130.684627	21.032794
73.887880	2137.703938	21.037811
73.941523	2133.781616	21.042829
74.346907	2119.831546	21.047847
73.959050	2129.676308	21.052864
74.020380	2131.252200	21.057882
74.702644	2131.305453	21.062899
74.670636	2138.368927	21.067917
74.962185	2159.742923	21.072935
74.691462	2150.085001	21.077952
74.972771	2136.763476	21.082970
75.064540	2160.799498	21.087987
74.761468	2142.597111	21.093005
75.250637	2160.906723	21.098023
75.036527	2141.398662	21.103040
74.707927	2153.302574	21.108058
75.578821	2146.777066	21.113075
75.115849	2149.186919	21.118093
75.509597	2119.808489	21.123111
75.373833	2162.839386	21.128128
75.147475	2131.272573	21.133146
75.085638	2163.936195	21.138163
74.883349	2154.684221	21.143181
75.547426	2152.910895	21.148199
75.398834	2173.740027	21.153216
75.782711	2148.297364	21.158234
75.739498	2169.888356	21.163251
76.232992	2140.012620	21.168269
76.128349	2186.099811	21.173287
76.108311	2184.824121	21.178304
75.908692	2156.827008	21.183322
76.136335	2202.778680	21.188339
75.727837	2186.330509	21.193357
76.837286	2162.493061	21.198375
76.516621	2155.020228	21.203392
76.590604	2179.065409	21.208410
76.596953	2205.164051	21.213427
76.566774	2195.985282	21.218445
77.010412	2151.029352	21.223463
76.801309	2198.633948	21.228480
76.828082	2198.686331	21.233498
77.172571	2161.898633	21.238515
77.044300	2205.820392	21.243533
77.133480	2171.324451	21.248551
77.097932	2184.974959	21.253568
77.701217	2205.521429	21.258586
77.814443	2200.724398	21.263603
77.420438	2185.577994	21.268621
77.711375	2177.271425	21.273639
77.594526	2194.088913	21.278656
77.823760	2203.343738	21.283674
78.023830	2205.352134	21.288691
77.953877	2214.797037	21.293709
77.801997	2186.719106	21.298727
78.068926	2229.485420	21.303744
77.581599	2198.978642	21.308762
78.431238	2174.474721	21.313779
78.149392	2202.477898	21.318797
78.232177	2214.413004	21.323815
78.175658	2187.582258	21.328832
78.381186	2198.465843	21.333850
78.325634	2211.809671	21.338867
78.106784	2201.923212	21.343885
78.670219	2202.029236	21.348903
78.620575	2232.138755	21.353920
78.684109	2210.783581	21.358938
78.738288	2201.152469	21.363955
78.447589	2237.669814	21.368973
78.750822	2230.331843	21.373991
78.905313	2229.144726	21.379008
78.636006	2257.742991	21.384026
79.003690	2232.356248	21.389043
78.767920	2268.924690	21.394061
79.535638	2244.862380	21.399079
79.971996	2268.511713	21.404096
79.766659	2290.808307	21.409114
79.874103	2255.585636	21.414131
80.531106	2238.850306	21.419149
79.875194	2258.014340	21.424167
79.657248	2228.384008	21.429184
80.101107	2232.096502	21.434202
80.367270	2278.481946	21.439219
80.259144	2277.180967	21.444237
80.194785	2256.104105	21.449255
80.279900	2230.219712	21.454272
80.192539	2268.487793	21.459290
80.728060	2290.081064	21.464307
80.383914	2255.710651	21.469325
80.755525	2231.728830	21.474343
80.545339	2267.494065	21.479360
80.190356	2287.511527	21.484378
80.201822	2254.420746	21.489395
80.103540	2290.867429	21.494413
80.537972	2284.371346	21.499431
81.087872	2284.179857	21.504448
80.890409	2308.016056	21.509466
81.437624	2289.850937	21.514483
81.077128	2285.149080	21.519501
81.157914	2302.565986	21.524519
81.554062	2291.621030	21.529536
81.370982	2314.482781	21.534554
81.764731	2325.545669	21.539571
81.461807	2318.117900	21.544589
81.572099	2323.894012	21.549607
82.125622	2319.444387	21.554624
81.976920	2297.565269	21.559642
82.278557	2304.905183	21.564659
82.334614	2289.981857	21.569677
82.223355	2315.470218	21.574695
82.713154	2291.229557	21.579712
82.646032	2333.122898	21.584730
82.445820	2290.086910	21.589747
82.128242	2297.511402	21.594765
82.411904	2316.164665	21.599783
82.436936	2295.586318	21.604800
82.545971	2279.999365	21.609818
82.798638	2330.919966	21.614835
82.585403	2314.964350	21.619853
83.277660	2299.945858	21.624871
83.198017	2351.013904	21.629888
82.915461	2327.414675	21.634906
82.943952	2351.809543	21.639923
83.193929	2329.651291	21.644941
83.045041	2334.995236	21.649959
83.205588	2343.010499	21.654976
83.157462	2335.302195	21.659994
83.831703	2350.036011	21.665011
83.571270	2360.275117	21.670029
83.540693	2370.066215	21.675047
84.032656	2356.025820	21.680064
83.685548	2367.770042	21.685082
84.105671	2358.479253	21.690099
83.762617	2370.204740	21.695117
83.648488	2365.747515	21.700135
84.419676	2374.438598	21.705152
84.055502	2389.994016	21.710170
84.341950	2381.163421	21.715187
84.366427	2403.067235	21.720205
84.604106	2394.646334	21.725223
84.648763	2382.301460	21.730240
84.595075	2384.243374	21.735258
84.708647	2383.828866	21.740275
85.049298	2384.729436	21.745293
85.227125	2409.434084	21.750311
85.499667	2394.732545	21.755328
85.755519	2394.296922	21.760346
85.944163	2345.050327	21.765363
85.538218	2370.001370	21.770381
85.817072	2362.883521	21.775399
85.826715	2357.049771	21.780416
85.802698	2353.226293	21.785434
85.638419	2357.392097	21.790451
85.424426	2378.093518	21.795469
85.630922	2356.911183	21.800487
85.664839	2343.691843	21.805504
85.463611	2363.425331	21.810522
85.869945	2361.562517	21.815539
85.705325	2393.187500	21.820557
85.913049	2387.290690	21.825575
85.980633	2378.175658	21.830592
85.947079	2387.577902	21.835610
85.997352	2398.565836	21.840627
86.338858	2420.221701	21.845645
86.426058	2426.699992	21.850663
86.685942	2410.359714	21.855680
86.762615	2427.889902	21.860698
86.742102	2416.308119	21.865715
86.798025	2419.962179	21.870733
86.842315	2442.466177	21.875751
86.899080	2455.867041	21.880768
87.177574	2433.376092	21.885786
87.396135	2449.031357	21.890803
87.464858	2445.539150	21.895821
87.530770	2437.733167	21.900839
87.863892	2432.904141	21.905856
87.285671	2454.324450	21.910874
88.019325	2431.736543	21.915891
88.187822	2469.358712	21.920909
88.264173	2435.937831	21.925927
88.004131	2451.695372	21.930944
87.753639	2449.308828	21.935962
88.271597	2441.223112	21.940979
88.431440	2466.237479	21.945997
88.472820	2462.533326	21.951015
88.874204	2453.487722	21.956032
88.521189	2458.240527	21.961050
88.691101	2486.371996	21.966067
88.549652	2460.839514	21.971085
88.413817	2475.790724	21.976103
88.992483	2445.538970	21.981120
88.687580	2486.397813	21.986138
89.123835	2446.564179	21.991155
89.205982	2490.096937	21.996173
89.322765	2471.351323	22.001191
89.420246	2505.122941	22.006208
89.782869	2484.997822	22.011226
89.886159	2474.450231	22.016243
89.698813	2474.364503	22.021261
89.478340	2476.705062	22.026279
89.798242	2483.342911	22.031296
89.652697	2486.059295	22.036314
89.742020	2481.977026	22.041331
89.569209	2486.813582	22.046349
89.567454	2488.451486	22.051367
89.702538	2479.945430	22.056384
89.940190	2492.401151	22.061402
90.260209	2489.065501	22.066419
90.076034	2500.095615	22.071437
90.134971	2510.207606	22.076455
90.490389	2493.655364	22.081472
90.348394	2505.690263	22.086490
90.187683	2513.012767	22.091507
90.415222	2527.320892	22.096525
90.685135	2536.215495	22.101543
90.886933	2531.960326	22.106560
90.770111	2532.798565	22.111578
91.045241	2552.161393	22.116595
91.320073	2543.807632	22.121613
91.523823	2552.518516	22.126631
92.137146	2538.364209	22.131648
91.470609	2555.167512	22.136666
91.621231	2539.045085	22.141683
91.927810	2545.054269	22.146701
91.931835	2522.012314	22.151719
92.086550	2552.355766	22.156736
92.126892	2525.729185	22.161754
92.274324	2529.138222	22.166771
92.398982	2547.457683	22.171789
92.419044	2528.286946	22.176807
92.328152	2538.827137	22.181824
92.331742	2527.468736	22.186842
92.142437	2554.841960	22.191859
92.553224	2531.566020	22.196877
92.388699	2571.609084	22.201895
92.599955	2557.927880	22.206912
92.541235	2588.311731	22.211930
93.180319	2559.628729	22.216947
92.872950	2561.343688	22.221965
92.958112	2592.963097	22.226983
93.535333	2582.077147	22.232000
93.341588	2588.003311	22.237018
93.593087	2596.636604	22.242035
93.743758	2581.668790	22.247053
93.462451	2572.064184	22.252071
93.640062	2588.539430	22.257088
93.867450	2588.387569	22.262106
93.749349	2577.688004	22.267123
93.865607	2592.813867	22.272141
93.596670	2613.458312	22.277159
94.435646	2606.491719	22.282176
94.047063	2613.670486	22.287194
94.147012	2615.539166	22.292211
94.256713	2622.227900	22.297229
94.055200	2611.753195	22.302247
94.495470	2632.001419	22.307264
95.008811	2648.098350	22.312282
94.814209	2640.623252	22.317299
95.159796	2643.883521	22.322317
94.922573	2640.970193	22.327335
95.438347	2633.785333	22.332352
95.230566	2647.502279	22.337370
95.298196	2635.873231	22.342387
95.681865	2634.103666	22.347405
95.230328	2641.126521	22.352423
95.322743	2640.937190	22.357440
95.424289	2634.261999	22.362458
95.344247	2635.709469	22.367475
95.566952	2654.906178	22.372493
95.537517	2672.761912	22.377511
95.870902	2661.442061	22.382528
96.071934	2668.159514	22.387546
96.340734	2661.611022	22.392563
96.658481	2658.065685	22.397581
96.451621	2658.136446	22.402599
96.367697	2648.316261	22.407616
96.642937	2663.856535	22.412634
96.410122	2649.360384	22.417651
96.550161	2656.628712	22.422669
96.685810	2687.697549	22.427687
97.211512	2674.056552	22.432704
97.176055	2694.911650	22.437722
96.812175	2674.449053	22.442739
97.171659	2686.057265	22.447757
96.842579	2705.955543	22.452775
97.469030	2693.994294	22.457792
97.337075	2715.302924	22.462810
97.775286	2709.293724	22.467827
97.713326	2698.039243	22.472845
97.799218	2717.535506	22.477863
98.317828	2712.195437	22.482880
98.067420	2702.302654	22.487898
97.940242	2699.224680	22.492915
97.916173	2694.251951	22.497933
97.805615	2719.885635	22.502951
98.242236	2735.884778	22.507968
98.575541	2734.495278	22.512986
98.324598	2722.962578	22.518003
98.514797	2738.750889	22.523021
98.504934	2744.100345	22.528039
98.901343	2745.088797	22.533056
99.136045	2757.141709	22.538074
99.049319	2768.711017	22.543091
99.622974	2766.943393	22.548109
99.455494	2766.133998	22.553127
99.475787	2756.412748	22.558144
99.463246	2753.571330	22.563162
99.528342	2755.583235	22.568179
99.874482	2756.800729	22.573197
99.611401	2768.553897	22.578215
99.487032	2759.993088	22.583232
99.524007	2762.967516	22.588250
99.631606	2782.648395	22.593267
100.188393	2778.268907	22.598285
100.226249	2778.684493	22.603303
100.195185	2787.985131	22.608320
100.584711	2779.811163	22.613338
100.441521	2782.617681	22.618355
100.803918	2776.354683	22.623373
100.879947	2782.625687	22.628391
100.816298	2775.153236	22.633408
101.062688	2763.378384	22.638426
100.781148	2763.900743	22.643443
100.267997	2772.384700	22.648461
100.899538	2806.631898	22.653479
101.155216	2786.908836	22.658496
101.408805	2794.848948	22.663514
101.178242	2801.422908	22.668531
101.629813	2803.362184	22.673549
101.488711	2822.601392	22.678567
102.230937	2812.867246	22.683584
102.416382	2815.043240	22.688602
102.210375	2832.180870	22.693619
102.248108	2822.984584	22.698637
102.535907	2817.065396	22.703655
102.318252	2817.554760	22.708672
102.428148	2836.208084	22.713690
102.441989	2809.316204	22.718707
102.892059	2818.435531	22.723725
102.828255	2823.444380	22.728743
102.726442	2826.024069	22.733760
102.832931	2805.743494	22.738778
102.744200	2814.225087	22.743795
103.041677	2816.917299	22.748813
103.009837	2832.291984	22.753831
103.227770	2833.016297	22.758848
103.393587	2852.684842	22.763866
103.152237	2852.326128	22.768883
103.118816	2848.047021	22.773901
102.943575	2845.515481	22.778919
102.999569	2862.546871	22.783936
103.412733	2872.467341	22.788954
103.248226	2897.766994	22.793971
104.337170	2891.878135	22.798989
104.025190	2896.864441	22.804007
104.354119	2892.329329	22.809024
104.222211	2902.533375	22.814042
104.618016	2892.214929	22.819059
105.066647	2881.477475	22.824077
104.780341	2886.758582	22.829095
104.862327	2914.629600	22.834112
105.151239	2907.034793	22.839130
105.147838	2923.415002	22.844147
105.118745	2921.153538	22.849165
105.204317	2915.419151	22.854183
105.433585	2921.023935	22.859200
105.419586	2927.739614	22.864218
105.559721	2909.155682	22.869235
105.682608	2911.804958	22.874253
105.670323	2913.473691	22.879271
105.877570	2907.122110	22.884288
105.891396	2920.675765	22.889306
105.972919	2912.503641	22.894323
105.965204	2902.347850	22.899341
106.330012	2916.953823	22.904359
106.232585	2925.132461	22.909376
106.120973	2918.056153	22.914394
106.253692	2932.757354	22.919411
106.759437	2934.713181	22.924429
106.394651	2941.303886	22.929447
106.348648	2940.162840	22.934464
106.638883	2950.166678	22.939482
106.512438	2964.338966	22.944499
106.961497	2954.188965	22.949517
106.897304	2978.157604	22.954535
107.251064	2992.357966	22.959552
107.880140	2981.395810	22.964570
107.618734	2983.237991	22.969587
108.100848	2979.358818	22.974605
108.103997	2988.264772	22.979623
108.003442	2976.681933	22.984640
108.506699	2971.392988	22.989658
108.197503	2975.820407	22.994675
108.097486	2983.022560	22.999693
108.213203	2989.189002	23.004711
108.554797	2965.480562	23.009728
108.434497	2987.488572	23.014746
107.961311	3000.297193	23.019763
108.723788	2999.134207	23.024781
108.632928	3007.159248	23.029799
108.974749	3013.732494	23.034816
109.169093	2986.515752	23.039834
108.871155	3021.656552	23.044851
109.243660	3011.138800	23.049869
109.277260	3031.481530	23.054887
109.168974	3045.085448	23.059904
109.713136	3014.573731	23.064922
109.372856	3051.394411	23.069939
110.248459	3025.836422	23.074957
110.155095	3075.628641	23.079975
109.653137	3036.473941	23.084992
110.221476	3078.356986	23.090010
110.254607	3060.210746	23.095027
110.296516	3054.490346	23.100045
110.363186	3065.151311	23.105063
110.608095	3056.872036	23.110080
110.757332	3055.128792	23.115098
110.645508	3088.791193	23.120115
111.172933	3087.323516	23.125133
111.234991	3073.122876	23.130151
111.170492	3111.028481	23.135168
111.093057	3081.561213	23.140186
111.180839	3082.285054	23.145203
111.303892	3095.715267	23.150221
111.299947	3060.247266	23.155239
111.012487	3113.804473	23.160256
111.487596	3083.808610	23.165274
111.597810	3122.818285	23.170291
111.887685	3119.910485	23.175309
111.949288	3090.476090	23.180327
111.956084	3135.506291	23.185344
112.390280	3120.954445	23.190362
112.413825	3158.983789	23.195379
112.329462	3135.112522	23.200397
112.759812	3158.238828	23.205415
112.977997	3134.107730	23.210432
113.121622	3133.520868	23.215450
113.104987	3138.104626	23.220467
113.285860	3121.507141	23.225485
113.802529	3142.477784	23.230503
113.771922	3129.031257	23.235520
113.616590	3122.036546	23.240538
113.540790	3136.639840	23.245555
113.906644	3139.894634	23.250573
113.614000	3127.798771	23.255591
113.505671	3139.011559	23.260608
114.054859	3127.863027	23.265626
113.876581	3147.059034	23.270643
114.140148	3147.270313	23.275661
114.271211	3130.193862	23.280679
114.063048	3151.796877	23.285696
114.678465	3149.328784	23.290714
114.432105	3136.928989	23.295731
114.671421	3164.084775	23.300749
114.791620	3162.245465	23.305767
114.743360	3163.295411	23.310784
114.796519	3173.605431	23.315802
115.230007	3179.740166	23.320819
115.076189	3169.225203	23.325837
115.458569	3207.472766	23.330855
115.028307	3202.979949	23.335872
115.762902	3166.949508	23.340890
115.670856	3229.441525	23.345907
115.574341	3204.378035	23.350925
116.488966	3205.510435	23.355943
115.871771	3231.891254	23.360960
116.347747	3236.132203	23.365978
116.136970	3229.840055	23.370995
116.266383	3210.367027	23.376013
116.599759	3244.466940	23.381031
116.263479	3213.948884	23.386048
116.578733	3241.205188	23.391066
116.680186	3233.470985	23.396083
116.963245	3220.082125	23.401101
116.958331	3264.483745	23.406119
116.626614	3251.551566	23.411136
117.227335	3260.344315	23.416154
117.728004	3267.605791	23.421171
117.486721	3287.930566	23.426189
117.860302	3270.918327	23.431207
117.879111	3276.924933	23.436224
117.616313	3283.295013	23.441242
117.885422	3259.194919	23.446259
117.691529	3300.818640	23.451277
117.588822	3294.933995	23.456295
118.245155	3285.626200	23.461312
118.672577	3267.893511	23.466330
118.370549	3327.575890	23.471347
118.289188	3319.975408	23.476365
118.734419	3297.310240	23.481383
118.782400	3328.944254	23.486400
118.770875	3338.036039	23.491418
119.183670	3308.166070	23.496435
119.421798	3355.513562	23.501453
119.933941	3331.926791	23.506471
119.695211	3361.853264	23.511488
119.797307	3332.321466	23.516506
120.184698	3365.448681	23.521523
120.127194	3329.049367	23.526541
120.378675	3361.066327	23.531559
119.937184	3345.387457	23.536576
120.175768	3323.441898	23.541594
120.169172	3363.041123	23.546611
120.279775	3326.747159	23.551629
120.705751	3341.842511	23.556647
120.794157	3367.355935	23.561664
120.936634	3350.146832	23.566682
120.874351	3372.440359	23.571699
120.732145	3385.970555	23.576717
120.834133	3374.980453	23.581735
120.798844	3374.750121	23.586752
121.399149	3385.428494	23.591770
121.136216	3401.793198	23.596787
121.290544	3413.180633	23.601805
121.721121	3412.735220	23.606823
121.698249	3421.865836	23.611840
122.021903	3453.567864	23.616858
122.283923	3420.621698	23.621875
122.255694	3418.267986	23.626893
122.412700	3434.175616	23.631911
122.706206	3413.552885	23.636928
122.613067	3433.593090	23.641946
122.704573	3440.936410	23.646963
122.852730	3439.625139	23.651981
123.191345	3441.313498	23.656999
122.749937	3443.870353	23.662016
123.152294	3428.609831	23.667034
123.283994	3457.133918	23.672051
123.289117	3470.402361	23.677069
123.785857	3472.627935	23.682087
124.203966	3467.808624	23.687104
124.048923	3466.481978	23.692122
124.292300	3471.588380	23.697139
124.393744	3466.325570	23.702157
124.517654	3465.003218	23.707175
124.584867	3468.727323	23.712192
124.069772	3467.764861	23.717210
124.714942	3460.717867	23.722227
124.453612	3459.943059	23.727245
124.887246	3464.682457	23.732263
124.703175	3473.033324	23.737280
125.060295	3473.643447	23.742298
124.702262	3463.797981	23.747315
124.836941	3507.413502	23.752333
124.895237	3486.671635	23.757351
124.635943	3496.288359	23.762368
124.981728	3529.997591	23.767386
125.670033	3529.883936	23.772403
125.647288	3535.147635	23.777421
125.967263	3543.036671	23.782439
126.090870	3548.300639	23.787456
126.193246	3541.628836	23.792474
126.595317	3540.292805	23.797491
126.382251	3544.793164	23.802509
126.790144	3543.213142	23.807527
126.582428	3569.009328	23.812544
126.907768	3576.124288	23.817562
126.983267	3567.297512	23.822579
127.066348	3577.609340	23.827597
127.258325	3574.843706	23.832615
127.301297	3585.896630	23.837632
127.548691	3591.052776	23.842650
127.712539	3603.954644	23.847667
127.364019	3616.438715	23.852685
127.886430	3596.944205	23.857703
127.573763	3611.461454	23.862720
128.023693	3603.776902	23.867738
128.382753	3634.539969	23.872755
128.202922	3643.809808	23.877773
128.560868	3624.806372	23.882791
128.581596	3640.159367	23.887808
128.577421	3633.211891	23.892826
129.061218	3634.251768	23.897843
128.753854	3646.854374	23.902861
129.310939	3643.439768	23.907879
129.220313	3641.288689	23.912896
129.024378	3660.256919	23.917914
129.710661	3644.862016	23.922931
129.725552	3697.237280	23.927949
130.135835	3647.947022	23.932967
130.179953	3690.345689	23.937984
129.963711	3666.568521	23.943002
130.197565	3675.094359	23.948019
130.035215	3679.927278	23.953037
130.426846	3661.350277	23.958055
130.492870	3671.781310	23.963072
130.638647	3690.017033	23.968090
130.999537	3686.164875	23.973107
130.909873	3720.534724	23.978125
131.050951	3680.957184	23.983143
131.138434	3704.207461	23.988160
130.995072	3705.997871	23.993178
131.064382	3685.722791	23.998195
131.328606	3732.772364	24.003213
131.123845	3727.127215	24.008231
131.545588	3696.010600	24.013248
131.427499	3747.719743	24.018266
132.270632	3755.655275	24.023283
132.124334	3736.162578	24.028301
131.792051	3771.809369	24.033319
132.289744	3746.912154	24.038336
132.248147	3794.213632	24.043354
132.968323	3763.022548	24.048371
132.794951	3793.126696	24.053389
133.208852	3780.024823	24.058407
133.048207	3767.566772	24.063424
133.126356	3798.835934	24.068442
133.326981	3775.630076	24.073459
133.242923	3818.656035	24.078477
133.638257	3795.707006	24.083495
133.640917	3812.708677	24.088512
133.865234	3787.913188	24.093530
134.010241	3826.924702	24.098547
134.346407	3821.341945	24.103565
134.826698	3819.149371	24.108583
135.075054	3838.795861	24.113600
135.076799	3827.779711	24.118618
135.198846	3803.566085	24.123635
135.315219	3840.632949	24.128653
135.582234	3808.730540	24.133671
135.190512	3836.407459	24.138688
135.538704	3812.607712	24.143706
135.714498	3816.002305	24.148723
135.516268	3817.604820	24.153741
135.558842	3824.364594	24.158759
135.577098	3800.583644	24.163776
135.147797	3834.964649	24.168794
135.495030	3827.319954	24.173811
135.364812	3834.917506	24.178829
136.088387	3856.185789	24.183847
136.401552	3881.784630	24.188864
136.386086	3867.439828	24.193882
136.330014	3895.016145	24.198899
136.375674	3877.496982	24.203917
136.607396	3907.650053	24.208935
136.911314	3914.180197	24.213952
136.651809	3903.252054	24.218970
136.895769	3944.268166	24.223987
137.384955	3928.611767	24.229005
137.510499	3948.112006	24.234023
138.022302	3944.750177	24.239040
138.031249	3944.876207	24.244058
138.491501	3963.265083	24.249075
138.157085	3940.858530	24.254093
138.684639	3952.843718	24.259111
139.014405	3958.200040	24.264128
138.677416	3954.393003	24.269146
139.247464	3936.304026	24.274163
139.148073	3951.099112	24.279181
139.742509	3923.016051	24.284199
139.663039	3965.213390	24.289216
139.263054	3941.679032	24.294234
139.729306	3922.803471	24.299251
139.323340	3952.440014	24.304269
139.497054	3923.461980	24.309287
139.626070	3951.181952	24.314304
139.616295	3931.889843	24.319322
139.601769	3962.679341	24.324339
140.090491	3955.094619	24.329357
140.346242	3956.201560	24.334375
140.173345	3954.940645	24.339392
140.212274	3994.181122	24.344410
140.985284	3982.250536	24.349427
141.098545	3993.409769	24.354445
141.161004	3984.747655	24.359463
141.393651	3984.106450	24.364480
141.221851	3982.407203	24.369498
141.570692	4001.756278	24.374515
141.896593	4006.853646	24.379533
141.452359	4013.595152	24.384551
141.571024	4023.920501	24.389568
141.799501	4003.866608	24.394586
142.235834	4010.732030	24.399603
142.254799	4042.239272	24.404621
142.480102	4039.250342	24.409639
142.659665	4033.273196	24.414656
142.499221	4037.646533	24.419674
142.584098	4024.423840	24.424691
142.691036	4056.194769	24.429709
142.765824	4063.159549	24.434727
142.919464	4063.378933	24.439744
143.013494	4073.046683	24.444762
143.857003	4081.754031	24.449779
143.696212	4092.776106	24.454797
143.553027	4085.699543	24.459815
144.236978	4087.432828	24.464832
144.075693	4128.609250	24.469850
144.276430	4122.411580	24.474867
144.607319	4111.386005	24.479885
144.883447	4114.715114	24.484903
144.873184	4105.963046	24.489920
144.774131	4119.015054	24.494938
145.395218	4120.431910	24.499955
145.592169	4126.100527	24.504973
145.521096	4117.586272	24.509991
145.578422	4119.155154	24.515008
145.709636	4142.329145	24.520026
145.878618	4125.434284	24.525043
145.854215	4127.078342	24.530061
145.980368	4128.514322	24.535079
146.018202	4137.560975	24.540096
145.760073	4129.419511	24.545114
145.806243	4133.188048	24.550131
146.270912	4159.630888	24.555149
146.040820	4162.921933	24.560167
146.406453	4153.173015	24.565184
146.344139	4185.301598	24.570202
146.902819	4191.838449	24.575219
146.804918	4193.339263	24.580237
147.155639	4209.864262	24.585255
147.556407	4225.306743	24.590272
147.722150	4214.547348	24.595290
147.931426	4210.125311	24.600307
147.893978	4230.307975	24.605325
148.064370	4227.209764	24.610343
148.304132	4228.060470	24.615360
148.773409	4237.733795	24.620378
148.844666	4226.773127	24.625395
148.871110	4222.446314	24.630413
148.800659	4237.493521	24.635431
149.199355	4253.631757	24.640448
149.089774	4254.447697	24.645466
149.159486	4269.110732	24.650483
149.675562	4254.444025	24.655501
149.277628	4260.837642	24.660519
149.746151	4267.981248	24.665536
149.888048	4286.005939	24.670554
149.750526	4282.591016	24.675571
150.027478	4274.886498	24.680589
150.464039	4315.758096	24.685607
150.547063	4304.126055	24.690624
150.484678	4316.754681	24.695642
150.910789	4325.673469	24.700659
151.099276	4291.488657	24.705677
150.814909	4323.086556	24.710695
151.433492	4330.792324	24.715712
151.455246	4350.725786	24.720730
151.350209	4340.977052	24.725747
151.606232	4347.833622	24.730765
151.922254	4342.205896	24.735783
152.091466	4360.509518	24.740800
151.967569	4369.533327	24.745818
152.330132	4365.686235	24.750835
152.896168	4369.696052	24.755853
152.767161	4369.305221	24.760871
152.864075	4353.784858	24.765888
152.777539	4376.045232	24.770906
153.147514	4385.479611	24.775923
152.987995	4398.234711	24.780941
153.479063	4394.522096	24.785959
153.672178	4391.317964	24.790976
153.210937	4383.329099	24.795994
153.567410	4418.123475	24.801011
154.170865	4400.982032	24.806029
153.538189	4441.974104	24.811047
154.367284	4421.159947	24.816064
154.532835	4418.056963	24.821082
154.288792	4417.955867	24.826099
154.775439	4424.627028	24.831117
154.958622	4420.542631	24.836135
155.306595	4443.717154	24.841152
155.050101	4423.266440	24.846170
154.859145	4455.464896	24.851187
155.184093	4422.846286	24.856205
155.320586	4452.743481	24.861223
155.262579	4482.017245	24.866240
155.392701	4450.495558	24.871258
155.752702	4504.463589	24.876275
155.982130	4471.976525	24.881293
155.948383	4513.508930	24.886311
156.451327	4507.752222	24.891328
156.853151	4520.413214	24.896346
156.666378	4504.606736	24.901363
156.724609	4531.769549	24.906381
156.862305	4518.183994	24.911399
157.269842	4549.151299	24.916416
157.608487	4549.706209	24.921434
157.562616	4539.758324	24.926451
157.702639	4547.156613	24.931469
158.063689	4576.263062	24.936487
158.595902	4571.510167	24.941504
158.588427	4568.335617	24.946522
158.752149	4568.012177	24.951539
158.702067	4577.925075	24.956557
158.521910	4556.991579	24.961575
158.578181	4574.871370	24.966592
159.027124	4588.452388	24.971610
159.256493	4585.473714	24.976627
159.178473	4599.727180	24.981645
159.269120	4601.061882	24.986663
159.526621	4608.153553	24.991680
159.915752	4625.357300	24.996698
159.980212	4625.928391	25.001715
160.387467	4614.448948	25.006733
160.232291	4642.667083	25.011751
160.584267	4608.330390	25.016768
160.516183	4650.420110	25.021786
161.103169	4649.700362	25.026803
161.240793	4647.259437	25.031821
160.530977	4645.772538	25.036839
160.889382	4665.419116	25.041856
161.259731	4670.646514	25.046874
160.916129	4686.573170	25.051891
161.850572	4676.549145	25.056909
161.435051	4696.053254	25.061927
161.556970	4718.634128	25.066944
161.999858	4700.964121	25.071962
161.895578	4707.211205	25.076979
162.458362	4739.495438	25.081997
162.764925	4735.984437	25.087015
162.741809	4727.096379	25.092032
162.844313	4754.586096	25.097050
162.945022	4738.226915	25.102067
163.151512	4758.894552	25.107085
163.461679	4776.886727	25.112103
163.662556	4764.394578	25.117120
163.717190	4762.701619	25.122138
163.907764	4769.495662	25.127155
164.231690	4785.025722	25.132173
164.304936	4786.995702	25.137191
164.648907	4784.410150	25.142208
164.382993	4786.781912	25.147226
164.719851	4801.102379	25.152243
165.094729	4776.200194	25.157261
165.410719	4800.081309	25.162279
165.537142	4810.941704	25.167296
165.519026	4807.956814	25.172314
165.960161	4801.541959	25.177331
166.267426	4798.206261	25.182349
166.005838	4801.370305	25.187367
166.282451	4805.261185	25.192384
166.457315	4800.325253	25.197402
166.636010	4804.291530	25.202419
166.871708	4803.999093	25.207437
166.076597	4821.405241	25.212455
166.490214	4834.628675	25.217472
166.613737	4835.178559	25.222490
166.836943	4845.234512	25.227507
167.162053	4865.109297	25.232525
167.418292	4859.431119	25.237543
167.737936	4869.207389	25.242560
167.531261	4885.981713	25.247578
167.470368	4892.661714	25.252595
168.011744	4892.468439	25.257613
168.396250	4910.590530	25.262631
168.252938	4911.017753	25.267648
168.330911	4913.180521	25.272666
168.585085	4937.597220	25.277683
168.789749	4954.918872	25.282701
168.952044	4948.198333	25.287719
169.182382	4960.936609	25.292736
169.585415	4986.533285	25.297754
169.415883	4971.536988	25.302771
170.058733	4969.574013	25.307789
169.829266	5000.040437	25.312807
170.462367	4995.693777	25.317824
170.499386	4987.605476	25.322842
170.641085	5001.064363	25.327859
171.094686	4980.690044	25.332877
170.704053	4983.275244	25.337895
170.950129	5001.584721	25.342912
171.623731	5004.512396	25.347930
171.227449	5016.879391	25.352947
171.512060	5007.444132	25.357965
171.415079	5008.748209	25.362983
171.518508	5023.818848	25.368000
171.988850	5034.459376	25.373018
171.746256	5038.239566	25.378035
172.109643	5045.485282	25.383053
172.064688	5051.299815	25.388071
172.473059	5077.401641	25.393088
172.876329	5063.438901	25.398106
172.649408	5065.531508	25.403123
173.153961	5094.200737	25.408141
173.451677	5094.327942	25.413159
174.000499	5081.665985	25.418176
174.099387	5079.107654	25.423194
174.267625	5084.227392	25.428211
174.675058	5072.545387	25.433229
174.529576	5089.730280	25.438247
174.745553	5097.279584	25.443264
174.626694	5112.118275	25.448282
174.610664	5115.775830	25.453299
175.130267	5115.527024	25.458317
174.845698	5109.362254	25.463335
174.958814	5148.977897	25.468352
175.163576	5129.399845	25.473370
175.257603	5137.885897	25.478387
175.651662	5152.599591	25.483405
175.625416	5179.087923	25.488423
175.700948	5176.378320	25.493440
176.189827	5177.340418	25.498458
176.359116	5198.029552	25.503475
176.689093	5192.185300	25.508493
176.731775	5202.480326	25.513511
177.031745	5222.492556	25.518528
177.319478	5219.375434	25.523546
177.241094	5225.587141	25.528563
177.576084	5229.308342	25.533581
177.817817	5249.317306	25.538599
177.898540	5239.969472	25.543616
178.050700	5264.555597	25.548634
177.909528	5250.692850	25.553651
178.450337	5258.778905	25.558669
178.427729	5276.078166	25.563687
178.452138	5280.969944	25.568704
179.115305	5304.670662	25.573722
179.185802	5304.690127	25.578739
179.376839	5304.690375	25.583757
179.689131	5304.816833	25.588775
179.311775	5309.306940	25.593792
179.829184	5309.959259	25.598810
179.796358	5342.741780	25.603827
179.709130	5337.838011	25.608845
180.015162	5346.225089	25.613863
180.372642	5353.876268	25.618880
180.619235	5365.303225	25.623898
180.651954	5377.215857	25.628915
180.923364	5380.458689	25.633933
181.165201	5395.416385	25.638951
181.159147	5403.568460	25.643968
181.380159	5402.280021	25.648986
181.397120	5424.586057	25.654003
181.854882	5423.701219	25.659021
181.791177	5430.955423	25.664039
182.494353	5432.058813	25.669056
182.818925	5438.103313	25.674074
182.725064	5440.795474	25.679092
182.897008	5445.220082	25.684109
183.481725	5441.965885	25.689127
182.851011	5450.360748	25.694144
183.556064	5469.465383	25.699162
183.639005	5473.921496	25.704180
183.490516	5477.262757	25.709197
183.602363	5478.369948	25.714215
183.867389	5493.745726	25.719232
184.218530	5498.761714	25.724250
183.920739	5508.922419	25.729268
184.301751	5526.285864	25.734285
184.563845	5527.721555	25.739303
184.829902	5552.569288	25.744320
185.507514	5542.177329	25.749338
185.377995	5553.544811	25.754356
185.687298	5553.318513	25.759373
185.761492	5571.030662	25.764391
185.792019	5592.393874	25.769408
186.086333	5584.239054	25.774426
186.066622	5595.922632	25.779444
186.426999	5610.240929	25.784461
186.674535	5611.678950	25.789479
186.864843	5617.704805	25.794496
187.117567	5632.119744	25.799514
187.078920	5639.399164	25.804532
187.571816	5641.694936	25.809549
187.625325	5640.496118	25.814567
187.750553	5658.104255	25.819584
188.027378	5664.196583	25.824602
187.829752	5670.890079	25.829620
188.277864	5679.758202	25.834637
188.518744	5699.866255	25.839655
188.485218	5701.838433	25.844672
188.921076	5701.086882	25.849690
188.966970	5694.265766	25.854708
189.236141	5721.764550	25.859725
189.313005	5724.402011	25.864743
189.437409	5738.359968	25.869760
190.131185	5753.768371	25.874778
189.755011	5749.067872	25.879796
189.886178	5755.229088	25.884813
190.460113	5770.810812	25.889831
190.074494	5782.870707	25.894848
190.776509	5778.447543	25.899866
190.774296	5794.261962	25.904884
191.043148	5801.412983	25.909901
191.390710	5821.686717	25.914919
191.255250	5813.853611	25.919936
191.744026	5827.320078	25.924954
191.809596	5838.492252	25.929972
191.732274	5841.856078	25.934989
192.066675	5851.430037	25.940007
191.760017	5867.644737	25.945024
192.433790	5863.125349	25.950042
192.692622	5883.012078	25.955060
192.855012	5890.901550	25.960077
193.170763	5890.739520	25.965095
193.299696	5903.969969	25.970112
193.740691	5917.522809	25.975130
193.930008	5926.291512	25.980148
194.125846	5928.858119	25.985165
194.586125	5924.228774	25.990183
194.472081	5931.747724	25.995200
194.831207	5939.418617	26.000218
194.653150	5953.219654	26.005236
194.860486	5944.495530	26.010253
195.319370	5968.949755	26.015271
195.360228	5973.440264	26.020288
195.641551	5961.711579	26.025306
195.466410	5980.897404	26.030324
195.613207	5994.031464	26.035341
196.142085	5994.568701	26.040359
196.097401	6003.637524	26.045376
196.110143	6022.533828	26.050394
196.326410	6034.604189	26.055412
196.850298	6037.802200	26.060429
197.010141	6045.880979	26.065447
196.907412	6057.091949	26.070464
197.485315	6058.128823	26.075482
197.692646	6088.645085	26.080500
198.023186	6085.705846	26.085517
198.374684	6084.111748	26.090535
198.356547	6084.827452	26.095552
198.776263	6097.551475	26.100570
198.867557	6112.656632	26.105588
199.225396	6121.071301	26.110605
199.575439	6113.105569	26.115623
199.144820	6122.208450	26.120640
199.792153	6119.807192	26.125658
199.651408	6140.806701	26.130676
199.935165	6137.661701	26.135693
200.455789	6131.117170	26.140711
200.381054	6145.264607	26.145728
200.425700	6152.597875	26.150746
200.619211	6172.190150	26.155764
201.011414	6161.641853	26.160781
201.274323	6163.119964	26.165799
201.283855	6177.076193	26.170816
201.623371	6193.649278	26.175834
201.770986	6184.715816	26.180852
201.325771	6202.438353	26.185869
201.743067	6202.907631	26.190887
201.880392	6203.437275	26.195904
202.224267	6220.763404	26.200922
202.369696	6215.142500	26.205940
202.490096	6235.186308	26.210957
202.998999	6262.353640	26.215975
202.896619	6255.866669	26.220992
203.133486	6245.322619	26.226010
203.679521	6275.073263	26.231028
203.792957	6283.605660	26.236045
204.174210	6277.404280	26.241063
204.099250	6301.695542	26.246080
204.469255	6316.215978	26.251098
204.532732	6315.861281	26.256116
204.556102	6314.980342	26.261133
204.740800	6330.771835	26.266151
204.740243	6337.948755	26.271168
205.043097	6364.727419	26.276186
205.379114	6371.908138	26.281204
205.393315	6389.822801	26.286221
206.177656	6398.087819	26.291239
206.119233	6396.096418	26.296256
206.391353	6416.734681	26.301274
206.597245	6427.387699	26.306292
206.761666	6426.097968	26.311309
207.350979	6438.110768	26.316327
207.097524	6449.666274	26.321344
207.387708	6458.873179	26.326362
207.824885	6458.671335	26.331380
207.788471	6482.174704	26.336397
208.195658	6482.057104	26.341415
208.555035	6485.728324	26.346432
208.487446	6480.459918	26.351450
208.906827	6496.193721	26.356468
208.870623	6515.701121	26.361485
209.110429	6492.139356	26.366503
209.026951	6517.075118	26.371520
209.596182	6541.142137	26.376538
209.818146	6529.903970	26.381556
209.840560	6551.313135	26.386573
210.219675	6559.412317	26.391591
210.485768	6564.677475	26.396608
210.783312	6565.197329	26.401626
211.286701	6592.187551	26.406644
211.589863	6595.231262	26.411661
211.328626	6594.047922	26.416679
211.244429	6607.811003	26.421696
211.588211	6611.832495	26.426714
211.813542	6601.626771	26.431732
211.991914	6612.309485	26.436749
212.270449	6623.247678	26.441767
212.597169	6632.282859	26.446784
212.528811	6642.888483	26.451802
212.646110	6640.676279	26.456820
212.661565	6653.015977	26.461837
213.185094	6656.859342	26.466855
213.131752	6672.909442	26.471872
213.403895	6682.501737	26.476890
213.795493	6696.221314	26.481908
213.498232	6694.444182	26.486925
214.330107	6719.032958	26.491943
214.294431	6736.512249	26.496960
214.792926	6735.387965	26.501978
214.815260	6749.565351	26.506996
215.021370	6762.362553	26.512013
215.500925	6760.514300	26.517031
215.289065	6781.356107	26.522048
215.881523	6787.437143	26.527066
216.044578	6780.879306	26.532084
216.081545	6798.631119	26.537101
216.641391	6829.610422	26.542119
216.916935	6821.801745	26.547136
216.940884	6817.595734	26.552154
217.059429	6830.665019	26.557172
217.366543	6852.262125	26.562189
217.653782	6848.803282	26.567207
217.660519	6855.964342	26.572224
217.887562	6868.926672	26.577242
217.876696	6891.724018	26.582260
218.267731	6894.059051	26.587277
218.278659	6896.095112	26.592295
218.459509	6926.331720	26.597312
218.704646	6930.272250	26.602330
218.985670	6923.975643	26.607348
219.427281	6971.059229	26.612365
219.422837	6960.832450	26.617383
220.148506	6962.496521	26.622400
220.133614	6999.977004	26.627418
220.881136	6985.700309	26.632436
220.590941	6996.486316	26.637453
220.987139	6995.914128	26.642471
221.203670	7001.519372	26.647488
221.497519	7017.484604	26.652506
221.523432	7031.145551	26.657524
221.546755	7026.662629	26.662541
222.405817	7034.660394	26.667559
222.076151	7063.560853	26.672576
221.998753	7046.170843	26.677594
222.641500	7081.543521	26.682612
222.850323	7057.145499	26.687629
222.566738	7108.177605	26.692647
222.986417	7089.203162	26.697664
223.248592	7118.834741	26.702682
223.475270	7120.106292	26.707700
223.587003	7145.960088	26.712717
224.325010	7139.999685	26.717735
224.307654	7183.666069	26.722752
224.641467	7166.063239	26.727770
224.885715	7170.141666	26.732788
224.675130	7187.804368	26.737805
225.015035	7185.492869	26.742823
225.241258	7203.397538	26.747840
225.467561	7206.468578	26.752858
225.642713	7217.155391	26.757876
225.547436	7240.338099	26.762893
225.700344	7252.850727	26.767911
226.225207	7254.754561	26.772928
226.342082	7275.272423	26.777946
226.871539	7286.157736	26.782964
226.958490	7309.103787	26.787981
227.355188	7313.935322	26.792999
227.621393	7308.050058	26.798016
227.687221	7347.062271	26.803034
228.162345	7329.930841	26.808052
227.939577	7368.496568	26.813069
228.645753	7356.854856	26.818087
228.700633	7364.638725	26.823104
228.686510	7391.146393	26.828122
229.431373	7383.425486	26.833140
229.232545	7415.141450	26.838157
229.509071	7415.694587	26.843175
229.830082	7446.935137	26.848192
229.971043	7454.260779	26.853210
230.252829	7443.168180	26.858228
230.235556	7479.352789	26.863245
231.100390	7468.884814	26.868263
231.381203	7469.079268	26.873280
231.426361	7505.081675	26.878298
231.604855	7483.743014	26.883316
231.854497	7507.871207	26.888333
232.193283	7525.677280	26.893351
232.313260	7515.756031	26.898368
232.487818	7528.584104	26.903386
233.050270	7531.205074	26.908404
233.298820	7553.314531	26.913421
233.217346	7550.671224	26.918439
233.290728	7561.077875	26.923456
233.325453	7581.010482	26.928474
233.731823	7565.086503	26.933492
233.867538	7606.116688	26.938509
234.248812	7602.470371	26.943527
234.480747	7608.067883	26.948544
234.366561	7640.273616	26.953562
235.005224	7640.242652	26.958580
235.419768	7662.213296	26.963597
235.553418	7657.329413	26.968615
235.541086	7672.540018	26.973632
235.723938	7672.808315	26.978650
235.921311	7706.254144	26.983668
236.373982	7719.509364	26.988685
236.642627	7728.347539	26.993703
236.792345	7721.191063	26.998720
236.667415	7746.375478	27.003738
237.576337	7748.874382	27.008756
237.453099	7745.744353	27.013773
237.329912	7780.549948	27.018791
238.025435	7771.638360	27.023808
237.920758	7778.396667	27.028826
238.215346	7812.921728	27.033844
238.584788	7814.959783	27.038861
238.878564	7795.537132	27.043879
238.970467	7836.745680	27.048896
239.275249	7847.244689	27.053914
239.869719	7852.898600	27.058932
239.910524	7870.979981	27.063949
239.573326	7868.310497	27.068967
240.069277	7889.583165	27.073984
240.059697	7909.206964	27.079002
240.580835	7918.069921	27.084020
241.051773	7930.648882	27.089037
240.968136	7950.895916	27.094055
241.439218	7954.676387	27.099072
241.590853	7967.921587	27.104090
242.349342	7994.849319	27.109108
242.212651	7997.380381	27.114125
242.605616	7990.772779	27.119143
243.175209	8023.107192	27.124160
243.263946	8000.448391	27.129178
243.243879	8027.378316	27.134196
243.733172	8020.745905	27.139213
243.775338	8042.900003	27.144231
244.559447	8039.611911	27.149248
244.323172	8042.197410	27.154266
244.928888	8063.957204	27.159284
244.909542	8054.232484	27.164301
245.018653	8071.828752	27.169319
245.788109	8065.002952	27.174336
245.810534	8112.162482	27.179354
246.077752	8070.464780	27.184372
246.072371	8114.382992	27.189389
246.018691	8110.081978	27.194407
246.671135	8094.163853	27.199424
246.631135	8105.923458	27.204442
247.040191	8165.698516	27.209460
247.210043	8169.748163	27.214477
246.737961	8158.047353	27.219495
247.555677	8155.372350	27.224512
247.403074	8212.660955	27.229530
247.895879	8188.469975	27.234548
248.205183	8251.011338	27.239565
248.021101	8239.497469	27.244583
248.973028	8228.465864	27.249600
249.015611	8258.574573	27.254618
249.255066	8295.739230	27.259636
249.146719	8295.781701	27.264653
249.635910	8291.789898	27.269671
250.145183	8337.084791	27.274688
249.979622	8326.937047	27.279706
250.859838	8337.509928	27.284724
250.917965	8347.748025	27.289741
251.273912	8342.084113	27.294759
251.354548	8375.853784	27.299776
251.465235	8359.186864	27.304794
251.906170	8396.440050	27.309812
252.251667	8364.918201	27.314829
252.015470	8411.511652	27.319847
252.445851	8412.026146	27.324864
252.592672	8448.529242	27.329882
252.409348	8434.630885	27.334900
253.153427	8431.985671	27.339917
253.243639	8494.170327	27.344935
253.546695	8480.357287	27.349952
253.595369	8503.693701	27.354970
253.869250	8499.748752	27.359988
254.177602	8541.684083	27.365005
254.830297	8521.768928	27.370023
255.261427	8575.122792	27.375040
255.064776	8567.921185	27.380058
255.662743	8594.143010	27.385076
256.358326	8597.555019	27.390093
256.399440	8590.650714	27.395111
256.657234	8613.541645	27.400128
256.753105	8614.424215	27.405146
256.930477	8624.268154	27.410164
257.326816	8643.275831	27.415181
257.393661	8631.723238	27.420199
257.643109	8678.302279	27.425216
257.877130	8655.050413	27.430234
258.323814	8695.890824	27.435252
258.619235	8681.400522	27.440269
258.273791	8716.904706	27.445287
258.969688	8696.560665	27.450304
258.647919	8747.699677	27.455322
259.523889	8746.403360	27.460340
259.828593	8752.189577	27.465357
259.573850	8796.204228	27.470375
259.966412	8773.116943	27.475392
260.214469	8827.942468	27.480410
260.827770	8824.837245	27.485428
261.147695	8832.094519	27.490445
261.331506	8827.286852	27.495463
262.173449	8850.591801	27.500480
262.085672	8856.243891	27.505498
262.306452	8871.461449	27.510516
262.834345	8864.095824	27.515533
262.587545	8893.614160	27.520551
262.834452	8886.416851	27.525568
263.347842	8897.349591	27.530586
263.331610	8898.845725	27.535604
263.486993	8939.567591	27.540621
263.475396	8959.796248	27.545639
263.987144	8948.690672	27.550656
263.956990	8963.922351	27.555674
264.672089	8973.400288	27.560692
264.670290	9003.311405	27.565709
264.723434	8999.032847	27.570727
265.033859	9012.115173	27.575744
265.119281	9023.933020	27.580762
265.385190	9052.953683	27.585780
265.794982	9066.335767	27.590797
265.741038	9085.725030	27.595815
266.610669	9095.331075	27.600832
266.457574	9130.036774	27.605850
267.070170	9131.723468	27.610868
267.562138	9135.893980	27.615885
267.740284	9140.908893	27.620903
268.344580	9172.350284	27.625920
268.411813	9177.389576	27.630938
268.877153	9170.400079	27.635956
269.443172	9181.351790	27.640973
268.990198	9217.842589	27.645991
269.736403	9183.910946	27.651008
269.419132	9217.160477	27.656026
269.952084	9238.969005	27.661044
270.037739	9236.947175	27.666061
270.480083	9261.129731	27.671079
270.520926	9276.719475	27.676096
270.701840	9293.492071	27.681114
271.257825	9295.128004	27.686132
271.598810	9310.992189	27.691149
271.652431	9331.751958	27.696167
272.222690	9337.523230	27.701184
272.181696	9355.685154	27.706202
272.471347	9365.928362	27.711220
272.976859	9376.591618	27.716237
273.073162	9391.556879	27.721255
273.563465	9414.228629	27.726272
273.697006	9418.154564	27.731290
274.214270	9436.775703	27.736308
274.463802	9430.542090	27.741325
274.271338	9453.745689	27.746343
274.706527	9471.620572	27.751360
275.017706	9486.051983	27.756378
275.311969	9505.262351	27.761396
275.640444	9495.940823	27.766413
275.729532	9521.840909	27.771431
276.103391	9549.241968	27.776448
276.486406	9527.202450	27.781466
276.634948	9581.996630	27.786484
276.914175	9561.441621	27.791501
277.018728	9610.520371	27.796519
277.526027	9603.784070	27.801536
277.406413	9628.222040	27.806554
277.681031	9655.127210	27.811572
278.558803	9654.977498	27.816589
278.320886	9667.314824	27.821607
278.616578	9691.730382	27.826624
279.225740	9703.615992	27.831642
279.361008	9723.332405	27.836660
280.050295	9721.760834	27.841677
279.755068	9755.916956	27.846695
280.243273	9732.744493	27.851712
280.637272	9752.957188	27.856730
280.533434	9779.245737	27.861748
281.023006	9792.029883	27.866765
281.358465	9790.548536	27.871783
281.531969	9811.214317	27.876800
281.920501	9834.808697	27.881818
281.965085	9832.471081	27.886836
282.111757	9844.727191	27.891853
282.224381	9876.679279	27.896871
282.583336	9900.933216	27.901888
283.057899	9908.259626	27.906906
283.213521	9931.489542	27.911924
283.921848	9945.258447	27.916941
284.211855	9947.643922	27.921959
284.394516	9964.253699	27.926976
284.749741	9989.262272	27.931994
284.902359	9994.968157	27.937012
285.624383	9997.811651	27.942029
285.450566	10027.086465	27.947047
285.980410	10027.946780	27.952064
286.394811	10057.753928	27.957082
286.353849	10072.183007	27.962100
286.497229	10067.354240	27.967117
287.045251	10109.373421	27.972135
287.338740	10121.213274	27.977152
287.796232	10126.218232	27.982170
287.865299	10138.307918	27.987188
288.266612	10149.928754	27.992205
288.484416	10172.180779	27.997223
288.553822	10189.891321	28.002240
289.337496	10191.358864	28.007258
289.396602	10219.769440	28.012276
290.040373	10225.907483	28.017293
290.122518	10245.171888	28.022311
290.354959	10245.251335	28.027328
290.568966	10256.088778	28.032346
290.570349	10288.545029	28.037364
291.426282	10281.136672	28.042381
291.026415	10291.024521	28.047399
291.505478	10328.381904	28.052416
292.334106	10340.273184	28.057434
291.996736	10360.961725	28.062452
292.089852	10369.738552	28.067469
292.494876	10385.570851	28.072487
292.932509	10404.745360	28.077504
292.993931	10423.516322	28.082522
293.240346	10438.006587	28.087540
293.666534	10442.631024	28.092557
294.124631	10483.556345	28.097575
294.637297	10485.964658	28.102592
295.111940	10493.237438	28.107610
294.926869	10501.518024	28.112628
295.285493	10514.061990	28.117645
295.692028	10527.620617	28.122663
295.714026	10542.337591	28.127680
295.971621	10553.390624	28.132698
296.123017	10574.461159	28.137716
296.872943	10582.969744	28.142733
296.953312	10619.652415	28.147751
296.955799	10628.355695	28.152768
297.595247	10641.104094	28.157786
297.643761	10667.168052	28.162804
297.877729	10699.304806	28.167821
298.249446	10695.704533	28.172839
298.553735	10708.396619	28.177856
298.993557	10754.956104	28.182874
298.993474	10755.286676	28.187892
299.570762	10784.944572	28.192909
300.058313	10786.182745	28.197927
300.453565	10808.272858	28.202944
300.767947	10836.349973	28.207962
300.608542	10849.893234	28.212980
300.816438	10854.067800	28.217997
301.201930	10871.321106	28.223015
301.608653	10912.839735	28.228032
302.267298	10925.979999	28.233050
302.514332	10927.292718	28.238068
302.982115	10956.045253	28.243085
302.858300	10953.692983	28.248103
303.183365	10976.634259	28.253120
303.973773	11002.384994	28.258138
303.967878	11013.974203	28.263156
304.103963	11014.095379	28.268173
304.631818	11056.118851	28.273191
305.009780	11050.447672	28.278208
305.135136	11063.145751	28.283226
305.428532	11105.862697	28.288244
305.863859	11093.022543	28.293261
306.074146	11110.763266	28.298279
306.234786	11144.838471	28.303296
306.431363	11161.270671	28.308314
306.614226	11171.491605	28.313332
307.397128	11197.606291	28.318349
307.592016	11210.465966	28.323367
307.840239	11252.931994	28.328384
308.272920	11242.886046	28.333402
308.476868	11265.330388	28.338420
309.072864	11305.969172	28.343437
309.589528	11288.916745	28.348455
309.554851	11322.031833	28.353472
310.079951	11327.779211	28.358490
310.461375	11323.021506	28.363508
310.339251	11370.851408	28.368525
310.875141	11365.162816	28.373543
310.903667	11377.355581	28.378560
311.549147	11392.111359	28.383578
311.806154	11410.240077	28.388596
311.936366	11415.590798	28.393613
312.343123	11428.895210	28.398631
312.275518	11449.327782	28.403648
312.740674	11456.353059	28.408666
313.175988	11465.654458	28.413684
312.978439	11501.389547	28.418701
313.746141	11485.568341	28.423719
313.787111	11537.800215	28.428736
314.503803	11537.928823	28.433754
314.431009	11552.727212	28.438772
314.867864	11587.920667	28.443789
315.160321	11573.205335	28.448807
315.076150	11627.325486	28.453824
315.711131	11626.122465	28.458842
315.704808	11669.033191	28.463860
316.191570	11681.377089	28.468877
316.760528	11716.415602	28.473895
317.338882	11726.180366	28.478912
317.490282	11731.336965	28.483930
317.428413	11776.203990	28.488948
318.092732	11762.467720	28.493965
318.394390	11809.894228	28.498983
318.769378	11808.789294	28.504000
319.513884	11820.804568	28.509018
319.664190	11832.531644	28.514036
319.977666	11853.468740	28.519053
320.337145	11867.280064	28.524071
320.399593	11885.748488	28.529088
321.199704	11887.147095	28.534106
321.489487	11919.447953	28.539124
321.578632	11920.779627	28.544141
321.761908	11931.635376	28.549159
321.758471	11954.225160	28.554176
321.948622	11974.296247	28.559194
322.039564	11988.855284	28.564212
322.642457	12025.280621	28.569229
323.197298	12041.262765	28.574247
323.259229	12069.105363	28.579264
323.931680	12079.904122	28.584282
324.252941	12111.148270	28.589300
324.550759	12125.152059	28.594317
325.068789	12144.159155	28.599335
325.270853	12156.004559	28.604352
325.619149	12180.649339	28.609370
325.888912	12202.808524	28.614388
326.127253	12217.361410	28.619405
326.388131	12239.487631	28.624423
326.565571	12257.968880	28.629440
326.994479	12273.366870	28.634458
327.155706	12293.101795	28.639476
327.797678	12313.300657	28.644493
328.328197	12334.265420	28.649511
328.428723	12352.717720	28.654528
328.650903	12369.678432	28.659546
329.192628	12390.849080	28.664564
329.514249	12394.573455	28.669581
330.061327	12412.547749	28.674599
330.184715	12424.586142	28.679616
330.668132	12433.491661	28.684634
330.751600	12456.932558	28.689652
331.101140	12471.126770	28.694669
331.360117	12474.061081	28.699687
331.569223	12508.384289	28.704704
331.835888	12516.850378	28.709722
331.908300	12520.230795	28.714740
332.144816	12559.654381	28.719757
332.634539	12583.560639	28.724775
332.870324	12608.141008	28.729792
333.081270	12633.544930	28.734810
333.517098	12665.487233	28.739828
333.798094	12686.606574	28.744845
334.469515	12703.960063	28.749863
334.702785	12740.946421	28.754880
334.948759	12750.094807	28.759898
335.252865	12775.471528	28.764916
335.852116	12805.241673	28.769933
336.297906	12813.517439	28.774951
336.499342	12849.657297	28.779968
337.034929	12861.772620	28.784986
337.728181	12880.435522	28.790004
337.649871	12896.210138	28.795021
338.193048	12910.332978	28.800039
338.374717	12943.294147	28.805056
338.412699	12954.670447	28.810074
338.943230	12984.275976	28.815092
339.183434	12997.272419	28.820109
340.016855	13013.419985	28.825127
340.040489	13039.172821	28.830144
340.761094	13039.732566	28.835162
340.753338	13063.959124	28.840180
340.858935	13084.562682	28.845197
341.330400	13096.913724	28.850215
341.821628	13127.184609	28.855232
342.162194	13152.568353	28.860250
342.459705	13174.464986	28.865268
342.897648	13186.074469	28.870285
343.444397	13214.454487	28.875303
343.187328	13242.132627	28.880320
343.736860	13244.208679	28.885338
344.126699	13266.121430	28.890356
344.387209	13298.681575	28.895373
344.876526	13308.549917	28.900391
345.000193	13332.459410	28.905408
345.675382	13355.239689	28.910426
346.084408	13372.635171	28.915444
346.225228	13391.421171	28.920461
346.791771	13398.422352	28.925479
347.188668	13423.156259	28.930496
347.531502	13434.080542	28.935514
348.037812	13442.764979	28.940532
348.076903	13456.146693	28.945549
348.437805	13454.426390	28.950567
348.304507	13487.237620	28.955584
348.725894	13505.553608	28.960602
348.977401	13512.498189	28.965620
349.254763	13541.630757	28.970637
349.789754	13558.414848	28.975655
349.849758	13586.747576	28.980672
350.216489	13599.520702	28.985690
350.778631	13632.853107	28.990708
350.828761	13665.103383	28.995725
351.262926	13684.935163	29.000743
351.387859	13706.938385	29.005760
351.966968	13736.662405	29.010778
352.620412	13765.446199	29.015796
352.827722	13790.275066	29.020813
353.522772	13808.799701	29.025831
353.532402	13836.141535	29.030848
353.937475	13858.339040	29.035866
354.597759	13890.274722	29.040884
354.719430	13885.315867	29.045901
355.199340	13926.678692	29.050919
355.467622	13958.546608	29.055936
355.947882	13969.928858	29.060954
356.021003	13977.165874	29.065972
356.270493	14009.279631	29.070989
357.389024	14024.407561	29.076007
357.220802	14056.118731	29.081024
358.095615	14073.554640	29.086042
358.422438	14085.463268	29.091060
358.501662	14115.368047	29.096077
359.202120	14126.973026	29.101095
359.341788	14140.163383	29.106112
359.564366	14156.606893	29.111130
359.972410	14182.924337	29.116148
360.380624	14201.621697	29.121165
361.006191	14217.478280	29.126183
361.244344	14243.465229	29.131200
361.395347	14252.986344	29.136218
361.808712	14271.250712	29.141236
361.736176	14299.124034	29.146253
362.370874	14322.022128	29.151271
362.735301	14351.843452	29.156288
362.848260	14368.687029	29.161306
363.370224	14395.476707	29.166324
363.498309	14422.543701	29.171341
364.054669	14446.319184	29.176359
364.418914	14471.513415	29.181376
364.553155	14491.709503	29.186394
365.016569	14526.213317	29.191412
365.397296	14553.443872	29.196429
365.988388	14568.794447	29.201447
366.163842	14598.966751	29.206464
366.480067	14597.507117	29.211482
366.782117	14618.755675	29.216500
367.396712	14653.739293	29.221517
367.792036	14658.863928	29.226535
368.150277	14678.443031	29.231552
368.169912	14706.587372	29.236570
368.881508	14719.810493	29.241588
368.883361	14760.167290	29.246605
369.279266	14773.011047	29.251623
369.720169	14807.281348	29.256640
370.145934	14822.756825	29.261658
370.783596	14847.365533	29.266676
370.882028	14867.820023	29.271693
371.596951	14882.162259	29.276711
371.793635	14912.096005	29.281728
371.851780	14929.763693	29.286746
372.490405	14938.197651	29.291764
373.053434	14965.430694	29.296781
373.662867	14975.142045	29.301799
374.306386	14993.359194	29.306816
374.564840	15004.584402	29.311834
374.825892	15035.197362	29.316852
375.015294	15045.484814	29.321869
375.775398	15065.056274	29.326887
376.171317	15084.048832	29.331904
376.082383	15090.112087	29.336922
376.984644	15105.438324	29.341940
376.808346	15132.167074	29.346957
377.314156	15174.928830	29.351975
377.562237	15151.553185	29.356992
377.603407	15203.537919	29.362010
378.167968	15211.300523	29.367028
378.465677	15244.077742	29.372045
378.957335	15275.150487	29.377063
379.241848	15278.823930	29.382080
379.742643	15318.152517	29.387098
380.167168	15312.235207	29.392116
380.547592	15369.456911	29.397133
381.124264	15373.619339	29.402151
381.218878	15408.465638	29.407168
381.965388	15415.547037	29.412186
382.468882	15455.713360	29.417204
382.446525	15464.012724	29.422221
383.005356	15457.165295	29.427239
383.228799	15537.423719	29.432256
382.996657	15538.269813	29.437274
384.423794	15551.428461	29.442292
384.137811	15584.744102	29.447309
384.822329	15581.433742	29.452327
384.956624	15613.859815	29.457344
385.254742	15646.043264	29.462362
385.778137	15664.670731	29.467380
386.098338	15696.545316	29.472397
386.602306	15737.245857	29.477415
387.304940	15734.742265	29.482432
387.280051	15755.470886	29.487450
387.841309	15758.481672	29.492468
387.978937	15800.593936	29.497485
388.239432	15825.957888	29.502503
388.783368	15828.213028	29.507520
389.020535	15866.827099	29.512538
389.477645	15885.243095	29.517556
389.822265	15903.459163	29.522573
390.011907	15939.197068	29.527591
390.577996	15972.964591	29.532608
390.475671	15987.026150	29.537626
391.305369	16024.060350	29.542644
391.423313	16048.126256	29.547661
391.845771	16077.317495	29.552679
392.459163	16095.899166	29.557696
392.878105	16127.968820	29.562714
393.648203	16144.840139	29.567732
393.711514	16165.747254	29.572749
394.340293	16200.316179	29.577767
394.862849	16232.548548	29.582784
395.083864	16244.091212	29.587802
395.765170	16265.379844	29.592820
395.952947	16274.494357	29.597837
396.255752	16315.578821	29.602855
396.620733	16329.981823	29.607872
397.018472	16354.912051	29.612890
397.804054	16379.053668	29.617908
397.879382	16422.272766	29.622925
398.258243	16429.159026	29.627943
398.802308	16448.471848	29.632960
398.820628	16476.166459	29.637978
399.816360	16502.354997	29.642996
400.391365	16546.008733	29.648013
400.593283	16547.214204	29.653031
400.888496	16569.125324	29.658048
400.581510	16607.202842	29.663066
401.718265	16623.550195	29.668084
401.733132	16647.884312	29.673101
401.961489	16681.470424	29.678119
402.709815	16712.996070	29.683136
402.587069	16745.707477	29.688154
403.155901	16759.446201	29.693172
403.788983	16782.655787	29.698189
403.871145	16822.894193	29.703207
404.111235	16854.672342	29.708224
404.804199	16887.837678	29.713242
405.320138	16912.976133	29.718260
405.864212	16933.549259	29.723277
406.381271	16975.413261	29.728295
407.193020	16983.326348	29.733312
407.364287	17005.203708	29.738330
407.709205	17016.904751	29.743348
408.070413	17053.037741	29.748365
409.078976	17066.037070	29.753383
409.428276	17074.789156	29.758400
409.418198	17101.312767	29.763418
409.991139	17105.187624	29.768436
410.227564	17120.436567	29.773453
410.487258	17137.263150	29.778471
410.820006	17167.415931	29.783488
411.051999	17188.153479	29.788506
411.777031	17207.170145	29.793524
412.116177	17214.128239	29.798541
412.511789	17244.813622	29.803559
413.067611	17257.457138	29.808576
413.151070	17276.096230	29.813594
413.514232	17308.065923	29.818612
413.904700	17341.639455	29.823629
413.866064	17348.811721	29.828647
414.210678	17405.205043	29.833664
414.488047	17416.137889	29.838682
415.274764	17466.968556	29.843700
415.564784	17473.472230	29.848717
415.511477	17528.658636	29.853735
416.158451	17571.435375	29.858752
416.682203	17600.769851	29.863770
417.340720	17645.714090	29.868788
417.733681	17670.618078	29.873805
418.148322	17701.969796	29.878823
418.969872	17743.034074	29.883840
419.336530	17753.770859	29.888858
419.598513	17785.578537	29.893876
419.784795	17826.483435	29.898893
420.633425	17825.307371	29.903911
421.015505	17882.677114	29.908928
421.318964	17899.538499	29.913946
421.874911	17919.420539	29.918964
422.610420	17948.444001	29.923981
422.978074	17978.562687	29.928999
423.613674	18003.022473	29.934016
423.957203	18025.491521	29.939034
424.335739	18056.320009	29.944052
424.583351	18081.674767	29.949069
424.938377	18107.604948	29.954087
425.509628	18131.338605	29.959104
425.574725	18167.989469	29.964122
426.096482	18191.811415	29.969140
426.847283	18202.615853	29.974157
426.950255	18251.878562	29.979175
427.734656	18265.814208	29.984192
427.996738	18295.044058	29.989210
428.384535	18310.631861	29.994228
428.670798	18342.522442	29.999245
428.991465	18377.548479	30.004263
429.918311	18395.495315	30.009280
429.809812	18442.200250	30.014298
430.356906	18458.361237	30.019316
430.813574	18493.642637	30.024333
430.904900	18524.943004	30.029351
431.524142	18554.600294	30.034368
432.111498	18576.084063	30.039386
432.193472	18606.819556	30.044404
432.650205	18634.643850	30.049421
432.884007	18669.896982	30.054439
433.408763	18697.818032	30.059456
433.725025	18721.116052	30.064474
434.389480	18758.430697	30.069492
434.501224	18800.554369	30.074509
435.109250	18832.495877	30.079527
435.666873	18852.388694	30.084544
436.045658	18884.123914	30.089562
436.407176	18922.373443	30.094580
436.616135	18947.382618	30.099597
437.183544	18978.247418	30.104615
437.532757	19014.268784	30.109632
437.819229	19050.789608	30.114650
438.319131	19080.784640	30.119668
439.138037	19124.831616	30.124685
439.344721	19165.577731	30.129703
440.199906	19195.194721	30.134720
440.755852	19222.575510	30.139738
441.040321	19257.229757	30.144756
441.678902	19288.366916	30.149773
441.805475	19323.999649	30.154791
442.628248	19343.801642	30.159808
442.617742	19383.259253	30.164826
443.226296	19416.917305	30.169844
444.055843	19448.576748	30.174861
443.959157	19483.510340	30.179879
444.916080	19501.497377	30.184896
445.076791	19534.539200	30.189914
445.439705	19568.258366	30.194932
445.918952	19598.892762	30.199949
446.466095	19640.876897	30.204967
447.005817	19656.036710	30.209984
447.537271	19696.007627	30.215002
448.117292	19723.807538	30.220020
448.459973	19755.034899	30.225037
448.900849	19789.782744	30.230055
449.331991	19814.716970	30.235072
449.805171	19842.283701	30.240090
450.219507	19869.349583	30.245108
450.743444	19904.764817	30.250125
451.121874	19935.882112	30.255143
451.430356	19967.353947	30.260160
451.687936	20012.081881	30.265178
452.344531	20020.921344	30.270196
453.089775	20045.295623	30.275213
453.433617	20088.296898	30.280231
454.093689	20112.762023	30.285248
454.429701	20138.152117	30.290266
454.423334	20171.340811	30.295284
455.243895	20199.532820	30.300301
455.535893	20231.429900	30.305319
455.970508	20244.996642	30.310336
456.355704	20290.451178	30.315354
456.969431	20315.147255	30.320372
457.312207	20331.529379	30.325389
457.558986	20368.076936	30.330407
458.200608	20384.909200	30.335424
458.448797	20415.637920	30.340442
458.758332	20450.456983	30.345460
459.229688	20485.754733	30.350477
459.299586	20517.623991	30.355495
460.276549	20550.872222	30.360512
460.557664	20582.080332	30.365530
460.780651	20628.892163	30.370548
461.732962	20656.517882	30.375565
461.889842	20692.944281	30.380583
462.475610	20733.019058	30.385600
463.174769	20760.980209	30.390618
463.603002	20795.312960	30.395636
464.115460	20821.182816	30.400653
464.727392	20864.625078	30.405671
465.085722	20889.412362	30.410688
465.524417	20918.957627	30.415706
465.738554	20964.452788	30.420724
466.488298	20971.074889	30.425741
467.139473	21022.638091	30.430759
467.480516	21045.374533	30.435776
468.308887	21077.831297	30.440794
468.444815	21109.165568	30.445812
468.848528	21145.053227	30.450829
469.206321	21175.584454	30.455847
469.856764	21201.254190	30.460864
470.391517	21238.834845	30.465882
470.360052	21271.972769	30.470900
470.957470	21300.600411	30.475917
471.213045	21350.890090	30.480935
472.108545	21378.721448	30.485952
472.467959	21422.781958	30.490970
473.218027	21463.371107	30.495988
473.653549	21483.027246	30.501005
473.491727	21519.578389	30.506023
474.289300	21552.079239	30.511040
474.976910	21593.954495	30.516058
475.273573	21643.426605	30.521076
475.929263	21669.794041	30.526093
476.239102	21693.164857	30.531111
476.835967	21731.273119	30.536128
477.366759	21772.446133	30.541146
477.810425	21790.841274	30.546164
478.724402	21822.689373	30.551181
478.922555	21862.956368	30.556199
479.531684	21884.960633	30.561216
480.354793	21907.085207	30.566234
480.533623	21947.149154	30.571252
481.128441	21963.820860	30.576269
481.453732	21992.055228	30.581287
481.816083	22023.107957	30.586304
482.126060	22053.664260	30.591322
482.678039	22081.197971	30.596340
483.185367	22100.219690	30.601357
483.370196	22129.972277	30.606375
483.796880	22164.303151	30.611392
484.555711	22188.032409	30.616410
485.052482	22221.832445	30.621428
485.429525	22252.755700	30.626445
486.084133	22280.842045	30.631463
486.644574	22306.639766	30.636480
486.787888	22334.187824	30.641498
487.450937	22371.611352	30.646516
488.088619	22390.958409	30.651533
488.364322	22421.867423	30.656551
488.841153	22452.731071	30.661568
489.340391	22491.419065	30.666586
489.593846	22529.011384	30.671604
490.180579	22559.226874	30.676621
490.886970	22593.666922	30.681639
491.149110	22634.078487	30.686656
491.897735	22658.595319	30.691674
492.370223	22699.745392	30.696692
493.052042	22724.747892	30.701709
493.454850	22754.758348	30.706727
493.790794	22782.874296	30.711744
494.204638	22820.741052	30.716762
494.405384	22862.036435	30.721780
495.093719	22885.781917	30.726797
495.782128	22929.080661	30.731815
496.105572	22967.545001	30.736832
496.554877	22995.927601	30.741850
497.239387	23034.088855	30.746868
497.667015	23070.746597	30.751885
497.950686	23124.020169	30.756903
498.602156	23163.106151	30.761920
499.283743	23179.908678	30.766938
499.888672	23224.399815	30.771956
500.287106	23261.072889	30.776973
501.126186	23289.923218	30.781991
501.632663	23330.007795	30.787008
502.246889	23365.344783	30.792026
502.621691	23393.601341	30.797044
503.193803	23416.572988	30.802061
503.355619	23440.694598	30.807079
503.503332	23498.472741	30.812096
504.595604	23490.238864	30.817114
504.461210	23565.050793	30.822132
505.450095	23579.541901	30.827149
505.719805	23610.991368	30.832167
506.285332	23656.250074	30.837184
507.052707	23691.815446	30.842202
507.343475	23730.684608	30.847220
507.927454	23755.370364	30.852237
508.282530	23796.337990	30.857255
508.896118	23832.692987	30.862272
509.374864	23858.318011	30.867290
510.038153	23879.587071	30.872308
510.249299	23926.056915	30.877325
510.663821	23943.321044	30.882343
511.067792	23980.260343	30.887360
511.475247	24011.922601	30.892378
511.908041	24037.144072	30.897396
512.449594	24090.507417	30.902413
513.239370	24131.514581	30.907431
513.382281	24159.725160	30.912448
513.727119	24208.856562	30.917466
514.093952	24257.842831	30.922484
514.631175	24290.748411	30.927501
515.297660	24337.937762	30.932519
516.050683	24383.046588	30.937536
516.682477	24413.994933	30.942554
517.110127	24469.158648	30.947572
517.629798	24501.642109	30.952589
517.954968	24536.353487	30.957607
518.556000	24584.430697	30.962624
519.607671	24615.788326	30.967642
519.637150	24662.265624	30.972660
520.366184	24698.293076	30.977677
520.995399	24735.639367	30.982695
521.554951	24777.769535	30.987712
522.104540	24809.193338	30.992730
522.527707	24858.888507	30.997748
523.023686	24891.664840	31.002765
523.413583	24932.787391	31.007783
523.716275	24990.519484	31.012800
524.608827	25017.243137	31.017818
525.321413	25056.114522	31.022836
525.739806	25098.313709	31.027853
526.393935	25147.113589	31.032871
526.873781	25183.464622	31.037888
527.713092	25214.693414	31.042906
527.707895	25251.038356	31.047924
528.313415	25285.016665	31.052941
529.202193	25326.111975	31.057959
529.444047	25365.437200	31.062976
530.119413	25405.439460	31.067994
530.251916	25444.536523	31.073012
531.045572	25498.272481	31.078029
531.531416	25541.540511	31.083047
531.726155	25578.518419	31.088064
532.457831	25602.048387	31.093082
532.638591	25655.292469	31.098100
533.227043	25704.107665	31.103117
534.061518	25736.584470	31.108135
534.593813	25794.295502	31.113152
535.912069	25815.237547	31.118170
536.254808	25846.756998	31.123188
536.383502	25902.698019	31.128205
536.894045	25940.532389	31.133223
537.421935	25968.064093	31.138240
537.972894	25990.145577	31.143258
538.390020	26042.935000	31.148276
538.927586	26076.710759	31.153293
539.423039	26094.406274	31.158311
539.943913	26152.250398	31.163328
540.202485	26177.341515	31.168346
540.750346	26226.259303	31.173364
541.335227	26262.106854	31.178381
542.067615	26305.536993	31.183399
542.900201	26339.736624	31.188416
543.370493	26369.768369	31.193434
543.613974	26416.506580	31.198452
544.504076	26436.095688	31.203469
545.335330	26462.505392	31.208487
545.821398	26501.833903	31.213504
546.476648	26533.119016	31.218522
546.858539	26581.570378	31.223540
547.367321	26619.679997	31.228557
547.656168	26651.778403	31.233575
548.342252	26687.984994	31.238592
548.716364	26727.335828	31.243610
548.850599	26773.676520	31.248628
549.765556	26820.810797	31.253645
550.438325	26852.625511	31.258663
550.813459	26902.730158	31.263680
551.565834	26935.628988	31.268698
551.797950	26986.093067	31.273716
552.264512	27036.577475	31.278733
553.066508	27065.602077	31.283751
553.753879	27108.508999	31.288768
554.139148	27140.815191	31.293786
554.658107	27215.180094	31.298804
555.074346	27243.590502	31.303821
555.896213	27281.870846	31.308839
556.104995	27325.907893	31.313856
556.913779	27381.562185	31.318874
557.499624	27434.506575	31.323892
558.106927	27454.941626	31.328909
559.080030	27511.191800	31.333927
559.530456	27555.436795	31.338944
560.365690	27584.572068	31.343962
560.281619	27616.271691	31.348980
560.820092	27656.194230	31.353997
561.856314	27709.040222	31.359015
562.319713	27743.478913	31.364032
562.916391	27783.736001	31.369050
563.600292	27830.754834	31.374068
563.754969	27875.655243	31.379085
564.607372	27907.095208	31.384103
565.018745	27950.305172	31.389120
565.707315	28000.103323	31.394138
566.009160	28024.868197	31.399156
566.372736	28093.789406	31.404173
567.428352	28108.715256	31.409191
567.487048	28152.757189	31.414208
568.364734	28197.560682	31.419226
568.922631	28216.713252	31.424244
569.196537	28277.676263	31.429261
569.981718	28289.314216	31.434279
570.164373	28339.784891	31.439296
571.029196	28388.125383	31.444314
571.660765	28425.986514	31.449332
572.183773	28450.077060	31.454349
572.693191	28484.926008	31.459367
573.160436	28524.663493	31.464384
573.651739	28566.065994	31.469402
574.461508	28621.634593	31.474420
574.871332	28667.241912	31.479437
575.331247	28713.181753	31.484455
575.770352	28762.377483	31.489472
576.890680	28802.318926	31.494490
577.265364	28842.168056	31.499508
577.383911	28890.205006	31.504525
578.239337	28941.794819	31.509543
578.794610	28989.579720	31.514560
579.351118	29026.890069	31.519578
579.964680	29082.264577	31.524596
580.429669	29145.135538	31.529613
581.120930	29175.005745	31.534631
581.530380	29235.968109	31.539648
582.480100	29277.520043	31.544666
583.142690	29325.027251	31.549684
583.358159	29366.385900	31.554701
584.004464	29432.428086	31.559719
584.636050	29466.678199	31.564736
585.209282	29515.575926	31.569754
585.971312	29573.508167	31.574772
586.273340	29621.434537	31.579789
587.364057	29648.596103	31.584807
587.842932	29734.736634	31.589824
588.626850	29755.842237	31.594842
589.246339	29798.618985	31.599860
589.402124	29867.719500	31.604877
590.489250	29884.377062	31.609895
590.805760	29926.364014	31.614912
591.314953	29982.574534	31.619930
592.091683	30025.670390	31.624948
592.847515	30072.156348	31.629965
593.218650	30115.000269	31.634983
593.786068	30156.783962	31.640000
594.493945	30207.085394	31.645018
595.246308	30246.554758	31.650036
595.555827	30297.922205	31.655053
596.470623	30333.528487	31.660071
596.898199	30380.636517	31.665088
597.701503	30430.248934	31.670106
598.401063	30463.675556	31.675124
598.695446	30512.166807	31.680141
599.596396	30536.814900	31.685159
599.620305	30589.330347	31.690176
600.384012	30626.414379	31.695194
601.071506	30641.254648	31.700212
601.350884	30702.652971	31.705229
602.034430	30737.010959	31.710247
602.904677	30799.606290	31.715264
602.696921	30826.842646	31.720282
603.149877	30883.489170	31.725300
603.777421	30919.093621	31.730317
604.737920	30985.150383	31.735335
605.594518	31042.633086	31.740352
605.964048	31083.049586	31.745370
606.397424	31120.192072	31.750388
606.631347	31196.374722	31.755405
607.740240	31228.238924	31.760423
608.114468	31281.224049	31.765440
608.854446	31338.354417	31.770458
609.567491	31376.039239	31.775476
610.238759	31442.596232	31.780493
610.661950	31501.342637	31.785511
611.686447	31541.843525	31.790528
612.213833	31598.910939	31.795546
612.903024	31648.171701	31.800564
613.153606	31705.285139	31.805581
614.281239	31742.047398	31.810599
614.827403	31787.897068	31.815616
615.433994	31852.878906	31.820634
615.981300	31885.937086	31.825652
616.603471	31938.389959	31.830669
617.243210	31996.205275	31.835687
618.125852	32038.957026	31.840704
618.569154	32079.573859	31.845722
619.244500	32133.878707	31.850740
619.753466	32188.159792	31.855757
620.499494	32232.539876	31.860775
620.712293	32271.903037	31.865792
621.299696	32343.865848	31.870810
622.050844	32384.193265	31.875828
622.498906	32438.529007	31.880845
623.341226	32488.314833	31.885863
624.128741	32554.734886	31.890880
624.598296	32596.195215	31.895898
625.427048	32661.641368	31.900916
625.729443	32706.708080	31.905933
626.229298	32757.616325	31.910951
626.893699	32827.340268	31.915968
628.047109	32853.523126	31.920986
628.395109	32938.966841	31.926004
629.013882	32958.537731	31.931021
629.629308	33026.230711	31.936039
630.399455	33072.289458	31.941056
630.906624	33129.363827	31.946074
632.000714	33164.303059	31.951092
632.242176	33230.379324	31.956109
632.804258	33238.705322	31.961127
633.705427	33283.072996	31.966144
634.272933	33369.291016	31.971162
635.002697	33383.097771	31.976180
635.286773	33448.578609	31.981197
636.187790	33474.753786	31.986215
636.761527	33542.937856	31.991232
637.282170	33553.808386	31.996250
638.150006	33601.990465	32.001268
638.597661	33655.803810	32.006285
639.151980	33700.535208	32.011303
640.078464	33752.130473	32.016320
640.363310	33780.790731	32.021338
640.886267	33845.990782	32.026356
641.765661	33897.609762	32.031373
642.459032	33932.180952	32.036391
642.834692	33996.697295	32.041408
643.418018	34056.551214	32.046426
644.287526	34099.803797	32.051444
644.681943	34160.511004	32.056461
645.218705	34204.824109	32.061479
646.054487	34259.832369	32.066496
646.561192	34318.941223	32.071514
647.339963	34363.164199	32.076532
647.421870	34428.706321	32.081549
648.423977	34480.219305	32.086567
649.236987	34535.320381	32.091584
649.747755	34598.135583	32.096602
650.950990	34651.248605	32.101620
651.643412	34713.168321	32.106637
651.908307	34754.879462	32.111655
652.556754	34821.928216	32.116672
653.255731	34869.010609	32.121690
653.898793	34933.158550	32.126708
654.395103	34985.924896	32.131725
655.285367	35028.602794	32.136743
655.886493	35097.255507	32.141760
656.525541	35166.277651	32.146778
657.612491	35195.151571	32.151796
658.152418	35255.669358	32.156813
658.470511	35305.375312	32.161831
659.419077	35358.181180	32.166848
659.860998	35431.876817	32.171866
660.944406	35464.932479	32.176884
661.424743	35508.726787	32.181901
662.071656	35578.179755	32.186919
663.170384	35632.340403	32.191936
663.234546	35664.508825	32.196954
664.085765	35734.454876	32.201972
664.661614	35771.347097	32.206989
665.047947	35832.104255	32.212007
665.789958	35903.904994	32.217024
666.505383	35956.939060	32.222042
667.116724	36013.891679	32.227060
667.880157	36072.940663	32.232077
668.729011	36118.221288	32.237095
669.356942	36167.279831	32.242112
669.608485	36228.050429	32.247130
670.781755	36250.574874	32.252148
671.676140	36301.951430	32.257165
672.142667	36359.353943	32.262183
672.524306	36389.119464	32.267200
672.835724	36460.073611	32.272218
674.152139	36497.068669	32.277236
674.104663	36543.368131	32.282253
674.993010	36615.003586	32.287271
675.816390	36653.430165	32.292288
676.063149	36707.938055	32.297306
676.940952	36774.653867	32.302324
677.470256	36815.717930	32.307341
677.860122	36899.486813	32.312359
678.690539	36955.581634	32.317376
679.287785	37005.684910	32.322394
680.473739	37070.650130	32.327412
681.244902	37151.334089	32.332429
681.839754	37180.474270	32.337447
682.980004	37239.666032	32.342464
683.478378	37307.946880	32.347482
684.232069	37344.995571	32.352500
684.895922	37420.961759	32.357517
685.626162	37465.254302	32.362535
686.157595	37511.763823	32.367552
686.861976	37580.482815	32.372570
687.761990	37625.967493	32.377588
688.486817	37690.794108	32.382605
688.899675	37749.628904	32.387623
689.651411	37800.764738	32.392640
690.078929	37855.853008	32.397658
691.033302	37907.612799	32.402676
691.664463	37959.335912	32.407693
692.112818	38032.084914	32.412711
693.090940	38087.262871	32.417728
693.506981	38151.145530	32.422746
694.480632	38215.575066	32.427764
695.177347	38282.447102	32.432781
695.651825	38325.481849	32.437799
696.416315	38385.661423	32.442816
696.972023	38448.378278	32.447834
698.009267	38496.487621	32.452852
698.656423	38581.871586	32.457869
699.706851	38624.793330	32.462887
699.908905	38689.276562	32.467904
700.517008	38764.929720	32.472922
701.473214	38801.728638	32.477940
702.183907	38864.712487	32.482957
702.607535	38936.838619	32.487975
703.874893	38983.411640	32.492992
704.377111	39047.233510	32.498010
705.047338	39107.559958	32.503028
706.119327	39144.970328	32.508045
706.383879	39216.925879	32.513063
707.322914	39251.503663	32.518080
707.475950	39305.358424	32.523098
708.124114	39357.295980	32.528116
708.896620	39417.755470	32.533133
709.042134	39486.703644	32.538151
710.065721	39549.506200	32.543168
710.663904	39592.270609	32.548186
711.327312	39664.211865	32.553204
712.017606	39738.498634	32.558221
712.443027	39790.733156	32.563239
713.758195	39867.174320	32.568256
714.220663	39905.132809	32.573274
715.288173	40001.143346	32.578292
715.706132	40030.239351	32.583309
716.706419	40121.043421	32.588327
717.404325	40151.843822	32.593344
717.868455	40245.152835	32.598362
718.580912	40299.456252	32.603380
719.279726	40376.898235	32.608397
719.838009	40428.492268	32.613415
721.218479	40502.115856	32.618432
721.794573	40555.046233	32.623450
722.673146	40618.634326	32.628468
723.420675	40685.077252	32.633485
723.923036	40747.577714	32.638503
725.028021	40810.324668	32.643520
725.988875	40861.291383	32.648538
726.709931	40914.947272	32.653556
727.596084	40979.413865	32.658573
728.143498	41040.146770	32.663591
729.131244	41097.179625	32.668608
729.441652	41152.670985	32.673626
729.994503	41206.411338	32.678644
730.889955	41264.210083	32.683661
731.450249	41327.610209	32.688679
732.436415	41377.229270	32.693696
733.146377	41453.906373	32.698714
733.354323	41529.253893	32.703732
734.256705	41586.437594	32.708749
735.137637	41652.743198	32.713767
735.563445	41709.441757	32.718784
736.041953	41772.462294	32.723802
736.781672	41852.094944	32.728820
738.468307	41908.975101	32.733837
738.741059	41976.012739	32.738855
739.632825	42053.035767	32.743872
740.101766	42109.649930	32.748890
741.118801	42170.460333	32.753908
742.319242	42232.844059	32.758925
742.706209	42297.959675	32.763943
743.475897	42355.637036	32.768960
744.085180	42440.923357	32.773978
745.148215	42488.716603	32.778996
745.683801	42531.793264	32.784013
746.400564	42595.822936	32.789031
746.933794	42664.638618	32.794048
747.964355	42717.351939	32.799066
748.390575	42771.035345	32.804084
749.014042	42807.783932	32.809101
749.720501	42893.612176	32.814119
750.705448	42945.298861	32.819136
751.140808	42991.304016	32.824154
751.590915	43058.055834	32.829172
752.603616	43123.115974	32.834189
752.864400	43205.878187	32.839207
753.892097	43263.006525	32.844224
754.618478	43334.699271	32.849242
755.243005	43400.670764	32.854260
756.619936	43464.251604	32.859277
756.765657	43536.687416	32.864295
757.274490	43624.071159	32.869312
758.215000	43685.312329	32.874330
758.944306	43755.075861	32.879348
760.018969	43822.381030	32.884365
760.297108	43903.500363	32.889383
761.188932	43989.295085	32.894400
762.477457	44055.182313	32.899418
762.973258	44124.180113	32.904436
763.953618	44194.060024	32.909453
764.609323	44280.584609	32.914471
765.876520	44332.053875	32.919488
766.531322	44406.418564	32.924506
767.153628	44482.006400	32.929524
767.918850	44546.685433	32.934541
768.665919	44619.175160	32.939559
769.587459	44684.665788	32.944576
770.494707	44760.739453	32.949594
771.108966	44837.468928	32.954612
771.804580	44902.990031	32.959629
772.602853	44966.889333	32.964647
773.747975	45043.368024	32.969664
774.223063	45103.186680	32.974682
774.855123	45162.825978	32.979700
775.982322	45255.409897	32.984717
776.197464	45327.375235	32.989735
776.990022	45388.895200	32.994752
777.665665	45461.330405	32.999770
778.770747	45538.208832	33.004788
779.789777	45608.798103	33.009805
780.061067	45711.454992	33.014823
781.408104	45755.483146	33.019840
781.989806	45820.057318	33.024858
782.291533	45914.779421	33.029876
783.643746	45983.020479	33.034893
784.131585	46054.368078	33.039911
784.653519	46133.168594	33.044928
785.732260	46208.183346	33.049946
786.461741	46287.787562	33.054964
787.429648	46350.961406	33.059981
787.772558	46414.096140	33.064999
789.091651	46490.739636	33.070016
789.710559	46565.497846	33.075034
790.316192	46627.124493	33.080052
791.845985	46688.752548	33.085069
792.437013	46756.515189	33.090087
793.039616	46807.974531	33.095104
793.855777	46884.393770	33.100122
794.246555	46941.534634	33.105140
795.190409	47011.687224	33.110157
795.716862	47077.558918	33.115175
796.638024	47137.774175	33.120192
797.119974	47219.359209	33.125210
797.839343	47303.304675	33.130228
798.866152	47379.591583	33.135245
799.678742	47440.544516	33.140263
800.204764	47539.120442	33.145280
801.146784	47610.891130	33.150298
802.025395	47686.376318	33.155316
802.867814	47764.978557	33.160333
803.444202	47842.689562	33.165351
804.187280	47930.183793	33.170368
805.264851	48001.076294	33.175386
805.992459	48097.247409	33.180404
806.931052	48171.816436	33.185421
807.415572	48239.718489	33.190439
807.892617	48339.887455	33.195456
809.055399	48423.366974	33.200474
809.997519	48500.019296	33.205492
810.872456	48579.935741	33.210509
811.809211	48677.054866	33.215527
812.453646	48744.109874	33.220544
813.734536	48822.378840	33.225562
814.158103	48922.322967	33.230580
815.241956	48987.526194	33.235597
816.041605	49071.946918	33.240615
816.823300	49162.640655	33.245632
817.574488	49225.657379	33.250650
818.577046	49327.856107	33.255668
819.374750	49410.331861	33.260685
820.486024	49493.184079	33.265703
821.008346	49555.632555	33.270720
821.816800	49641.553433	33.275738
822.226818	49725.117878	33.280756
823.671392	49793.280156	33.285773
824.775116	49874.081126	33.290791
825.464518	49949.486184	33.295808
826.241837	50033.353354	33.300826
827.216324	50119.063940	33.305844
828.169998	50178.422934	33.310861
828.836794	50252.384469	33.315879
829.573292	50322.990290	33.320896
830.523468	50419.706595	33.325914
831.092451	50494.060218	33.330932
832.205152	50565.058381	33.335949
832.900920	50619.795864	33.340967
833.795487	50713.341723	33.345984
834.347697	50776.174718	33.351002
834.956022	50840.226564	33.356020
835.998785	50906.367999	33.361037
836.687269	50968.479419	33.366055
837.380230	51048.451715	33.371072
838.574828	51134.662321	33.376090
838.805173	51199.804380	33.381108
839.813933	51283.018914	33.386125
840.512884	51372.424282	33.391143
841.350717	51444.832988	33.396160
842.221181	51519.553154	33.401178
843.115755	51595.945534	33.406196
844.018204	51685.058146	33.411213
844.810004	51776.735579	33.416231
845.583925	51852.390850	33.421248
846.727421	51932.371139	33.426266
847.348879	52022.205501	33.431284
847.971606	52107.659710	33.436301
849.050364	52203.213294	33.441319
849.787320	52279.472718	33.446336
850.734642	52364.740789	33.451354
851.724379	52448.591799	33.456372
852.638094	52544.141901	33.461389
853.518542	52614.948466	33.466407
854.371139	52700.854938	33.471424
855.556880	52783.489658	33.476442
856.235049	52879.880657	33.481460
857.121395	52939.325811	33.486477
858.433348	53018.059580	33.491495
859.167504	53096.184990	33.496512
860.019915	53175.043072	33.501530
860.574130	53269.524349	33.506548
861.773693	53342.397588	33.511565
862.517649	53427.886112	33.516583
863.079299	53512.353053	33.521600
864.391556	53573.471563	33.526618
864.730730	53695.605740	33.531636
865.817292	53746.291689	33.536653
866.825204	53843.455970	33.541671
867.446417	53935.057911	33.546688
868.376120	54012.726920	33.551706
869.042132	54091.915351	33.556724
870.145327	54184.000510	33.561741
871.056793	54275.778924	33.566759
871.508430	54361.867569	33.571776
873.012791	54435.204878	33.576794
873.638559	54528.579785	33.581812
873.933454	54605.708459	33.586829
875.095548	54725.692246	33.591847
875.955705	54801.611293	33.596864
877.098025	54882.573860	33.601882
877.753441	54976.659694	33.606900
878.929398	55055.976349	33.611917
879.848960	55131.893637	33.616935
880.365914	55228.752060	33.621952
881.652663	55305.381816	33.626970
882.341954	55362.969254	33.631988
882.908616	55448.615456	33.637005
884.223877	55512.896527	33.642023
884.701446	55615.233484	33.647040
885.928207	55676.833551	33.652058
886.674834	55749.876926	33.657076
887.512079	55839.683264	33.662093
888.842140	55913.657182	33.667111
889.109144	56009.691464	33.672128
890.397480	56084.054660	33.677146
890.958073	56162.934274	33.682164
891.802730	56251.415678	33.687181
892.426366	56345.709336	33.692199
893.278066	56428.467481	33.697216
894.311378	56512.147261	33.702234
895.016368	56618.775127	33.707252
896.018387	56706.753874	33.712269
897.067637	56797.134106	33.717287
897.994776	56883.963945	33.722304
898.796179	56967.802662	33.727322
899.502038	57083.016292	33.732340
900.525314	57167.193114	33.737357
901.594075	57258.885738	33.742375
902.732294	57362.450026	33.747392
903.707879	57452.365369	33.752410
904.474320	57541.162178	33.757428
905.753367	57647.101710	33.762445
906.557412	57700.514334	33.767463
907.506396	57831.396269	33.772480
908.577828	57873.528296	33.777498
909.280642	57990.364422	33.782516
910.500956	58060.869755	33.787533
911.602618	58140.442056	33.792551
912.327812	58251.132845	33.797568
913.240007	58304.697333	33.802586
913.764036	58413.255412	33.807604
914.979311	58484.066237	33.812621
915.654788	58573.965344	33.817639
916.286470	58687.082430	33.822656
917.617187	58763.615465	33.827674
918.396615	58858.759073	33.832692
919.270581	58967.848782	33.837709
920.093632	59065.947864	33.842727
921.252156	59115.589109	33.847744
922.220844	59245.151921	33.852762
923.007554	59320.062644	33.857780
923.371953	59429.542386	33.862797
925.072131	59496.854406	33.867815
925.818701	59632.611765	33.872832
926.725204	59673.375502	33.877850
927.722636	59795.824383	33.882868
928.858626	59869.854556	33.887885
930.014691	59952.933688	33.892903
930.600212	60054.741359	33.897920
931.552536	60117.366088	33.902938
932.269821	60198.928015	33.907956
933.077277	60281.956732	33.912973
934.242289	60367.568457	33.917991
934.734074	60446.840394	33.923008
935.636502	60531.481143	33.928026
936.437796	60640.525914	33.933044
937.215389	60712.747292	33.938061
938.166044	60820.515867	33.943079
939.085489	60921.949923	33.948096
940.054603	61010.402712	33.953114
940.854857	61111.822029	33.958132
941.773888	61212.683069	33.963149
942.656178	61292.777393	33.968167
943.412758	61416.007748	33.973184
944.663592	61514.765246	33.978202
945.689882	61610.982437	33.983220
946.123886	61723.006349	33.988237
947.131596	61831.365278	33.993255
948.398444	61927.495297	33.998272
949.557886	62037.182722	34.003290
950.510781	62143.556562	34.008308
951.364634	62253.887501	34.013325
952.668117	62338.968354	34.018343
953.396315	62439.332694	34.023360
954.506678	62557.484062	34.028378
955.539286	62657.820081	34.033396
956.279021	62740.731515	34.038413
957.319437	62856.388646	34.043431
957.904888	62963.447644	34.048448
959.405414	63042.339528	34.053466
960.476138	63176.858372	34.058484
961.536434	63255.669610	34.063501
962.489597	63377.814173	34.068519
963.623745	63448.340943	34.073536
964.526223	63560.983324	34.078554
965.815842	63649.400680	34.083572
966.256126	63747.098831	34.088589
967.667753	63865.879919	34.093607
968.392367	63965.033967	34.098624
969.594322	64053.764002	34.103642
970.298160	64137.549382	34.108660
971.165918	64265.261780	34.113677
972.673542	64352.141374	34.118695
973.350471	64458.227907	34.123712
974.219700	64540.580277	34.128730
975.490525	64663.794200	34.133748
976.096279	64731.599140	34.138765
977.034501	64866.694218	34.143783
977.586538	64944.367989	34.148800
978.648220	65033.020690	34.153818
979.749764	65186.475403	34.158836
980.734613	65270.085258	34.163853
981.415154	65381.870489	34.168871
982.513439	65470.001457	34.173888
983.480798	65572.744523	34.178906
984.440068	65680.356235	34.183924
985.098866	65767.149923	34.188941
986.145105	65866.966975	34.193959
987.307484	65997.426499	34.198976
988.030555	66070.115994	34.203994
988.783587	66183.141887	34.209012
989.798385	66299.193527	34.214029
990.931015	66392.139706	34.219047
992.066680	66505.172949	34.224064
992.486683	66621.422220	34.229082
994.241688	66732.295860	34.234100
994.900623	66834.384106	34.239117
995.844489	66936.487576	34.244135
997.293693	67048.817184	34.249152
998.181020	67167.537952	34.254170
999.286981	67272.640063	34.259188
1000.188051	67393.997364	34.264205
1001.136568	67485.417814	34.269223
1002.110265	67608.394700	34.274240
1002.830891	67732.417044	34.279258
1004.232813	67827.696226	34.284276
1004.990489	67948.031169	34.289293
1006.461749	68072.751203	34.294311
1007.449578	68177.466406	34.299328
1008.349969	68285.146253	34.304346
1009.504372	68394.093975	34.309364
1010.410014	68514.813207	34.314381
1011.678576	68623.535586	34.319399
1012.713140	68733.376076	34.324416
1013.769888	68845.393182	34.329434
1014.972138	68969.517391	34.334452
1015.726768	69056.945527	34.339469
1016.521723	69179.512257	34.344487
1017.216937	69310.100036	34.349504
1018.517746	69386.728104	34.354522
1019.699491	69538.290400	34.359540
1020.802920	69638.894904	34.364557
1021.826336	69745.388164	34.369575
1022.850853	69857.631018	34.374592
1023.840807	69994.494280	34.379610
1025.061452	70081.031558	34.384628
1025.920344	70223.413808	34.389645
1027.312524	70285.120615	34.394663
1028.275790	70445.203351	34.399680
1028.890261	70543.394681	34.404698
1030.398847	70622.490164	34.409716
1031.022571	70766.518544	34.414733
1032.109632	70879.123750	34.419751
1033.575204	70977.181871	34.424768
1034.347389	71098.652241	34.429786
1035.487442	71209.980957	34.434804
1036.390144	71311.396799	34.439821
1037.469523	71441.267932	34.444839
1038.264860	71523.380594	34.449856
1039.147452	71642.960216	34.454874
1040.562794	71709.899430	34.459892
1041.238023	71859.885847	34.464909
1042.492770	71922.163050	34.469927
1043.541829	72062.272670	34.474944
1044.298206	72138.075591	34.479962
1045.481978	72274.620598	34.484980
1046.408080	72344.400998	34.489997
1047.611406	72474.796292	34.495015
1047.894441	72592.821539	34.500032
1048.820180	72681.072653	34.505050
1050.102164	72824.366831	34.510068
1051.022492	72959.713668	34.515085
1051.992517	73057.412313	34.520103
1053.381949	73191.599281	34.525120
1054.205778	73290.554502	34.530138
1055.563016	73439.622932	34.535156
1056.391665	73534.382827	34.540173
1057.479060	73690.642805	34.545191
1058.174742	73782.644662	34.550208
1059.197512	73946.139587	34.555226
1060.776134	74040.011673	34.560244
1061.748829	74202.278111	34.565261
1063.143860	74322.601219	34.570279
1063.761443	74436.103846	34.575296
1065.257009	74551.003062	34.580314
1066.261660	74704.402533	34.585332
1067.044018	74804.003784	34.590349
1068.447767	74962.428843	34.595367
1069.386046	75067.713039	34.600384
1070.416319	75185.432538	34.605402
1071.667214	75309.538274	34.610420
1072.681618	75456.268521	34.615437
1073.955796	75582.160676	34.620455
1075.110718	75703.623552	34.625472
1076.132666	75825.392697	34.630490
1077.325721	75964.400857	34.635508
1078.513218	76085.930375	34.640525
1079.502715	76195.813118	34.645543
1080.705827	76335.681730	34.650560
1080.942636	76472.665125	34.655578
1082.780630	76562.791675	34.660596
1083.435311	76728.870461	34.665613
1085.099698	76846.947529	34.670631
1086.091180	76956.992092	34.675648
1087.107546	77100.940519	34.680666
1088.495384	77214.709177	34.685684
1089.296078	77329.955965	34.690701
1090.436494	77468.685783	34.695719
1091.784456	77578.120844	34.700736
1092.767942	77713.944707	34.705754
1094.191466	77843.486623	34.710772
1095.248719	77951.516256	34.715789
1095.818898	78063.656326	34.720807
1097.173296	78198.615424	34.725824
1098.099313	78290.108216	34.730842
1099.265721	78398.843392	34.735860
1100.527462	78529.192816	34.740877
1101.487235	78627.602731	34.745895
1102.354940	78726.634539	34.750912
1103.006820	78871.209649	34.755930
1104.628477	78958.138760	34.760948
1105.079475	79103.398483	34.765965
1106.147183	79221.660070	34.770983
1107.321197	79333.186449	34.776000
1108.292633	79488.700601	34.781018
1109.586057	79584.154473	34.786036
1110.592267	79746.270334	34.791053
1111.953700	79865.266389	34.796071
1113.056798	80015.188517	34.801088
1113.995262	80106.529416	34.806106
1115.435784	80266.873636	34.811124
1116.535278	80367.981411	34.816141
1117.722506	80531.869856	34.821159
1118.419948	80643.972177	34.826176
1119.650984	80800.162913	34.831194
1120.794189	80909.800044	34.836212
1122.253656	81064.407742	34.841229
1122.903230	81172.525474	34.846247
1124.165387	81335.346383	34.851264
1125.330422	81458.276826	34.856282
1126.693933	81599.072501	34.861300
1127.584961	81732.194097	34.866317
1128.603032	81861.143086	34.871335
1130.003013	82015.887443	34.876352
1131.271943	82140.777741	34.881370
1132.407102	82295.496751	34.886388
1133.662158	82418.601887	34.891405
1134.752190	82549.117799	34.896423
1135.733447	82690.101754	34.901440
1136.612532	82838.954633	34.906458
1138.310963	82964.590762	34.911476
1139.236534	83097.993745	34.916493
1140.396690	83241.507024	34.921511
1141.441824	83388.276445	34.926528
1142.767625	83504.365620	34.931546
1144.007855	83655.657760	34.936564
1144.983582	83789.702021	34.941581
1146.199465	83917.405748	34.946599
1147.827855	84054.275078	34.951616
1148.693334	84203.506490	34.956634
1150.205141	84322.554716	34.961652
1151.389541	84446.169817	34.966669
1152.189038	84579.324070	34.971687
1153.286186	84720.929146	34.976704
1154.608712	84845.264344	34.981722
1155.752438	84969.439031	34.986740
1157.104404	85116.519446	34.991757
1157.640510	85248.031678	34.996775
1159.260822	85359.702716	35.001792
1160.079084	85473.771701	35.006810
1161.558982	85606.798942	35.011828
1163.262316	85717.503945	35.016845
1163.814777	85839.103242	35.021863
1165.434724	85948.362157	35.026880
1166.128957	86073.790823	35.031898
1167.813395	86191.608146	35.036916
1168.653626	86297.799800	35.041933
1169.767359	86442.916616	35.046951
1170.622367	86527.975881	35.051968
1171.567076	86682.795313	35.056986
1172.764459	86795.704584	35.062004
1173.956281	86952.263448	35.067021
1175.102459	87049.532610	35.072039
1176.320258	87218.646973	35.077056
1177.237490	87332.406665	35.082074
1178.545818	87481.122776	35.087092
1179.503901	87623.806300	35.092109
1180.524895	87749.622831	35.097127
1182.141007	87905.792392	35.102144
1183.419762	88022.192009	35.107162
1184.569322	88196.004233	35.112180
1186.062779	88313.882595	35.117197
1186.929264	88447.202120	35.122215
1188.378243	88595.454614	35.127232
1189.574857	88732.637696	35.132250
1190.689223	88869.682960	35.137268
1191.834080	89009.961966	35.142285
1193.120433	89144.654518	35.147303
1194.122941	89293.716344	35.152320
1195.310030	89426.270030	35.157338
1196.384998	89579.850144	35.162356
1198.043682	89699.638578	35.167373
1198.716517	89850.995304	35.172391
1199.928528	90017.514442	35.177408
1201.357817	90149.509152	35.182426
1202.388033	90299.939470	35.187444
1203.962782	90448.184653	35.192461
1204.856297	90605.000851	35.197479
1207.047608	90705.611263	35.202496
1208.110134	90888.091411	35.207514
1209.158528	90985.121914	35.212532
1210.232811	91165.262536	35.217549
1211.018074	91283.535264	35.222567
1212.717207	91441.804146	35.227584
1213.840238	91571.610998	35.232602
1215.324275	91716.046616	35.237620
1216.377974	91853.942500	35.242637
1217.518366	91987.771438	35.247655
1219.372158	92131.177025	35.252672
1220.265538	92280.346178	35.257690
1221.165919	92392.351531	35.262708
1222.636777	92555.654890	35.267725
1224.287464	92665.240157	35.272743
1225.337087	92816.228595	35.277760
1226.519037	92916.876830	35.282778
1227.583762	93063.551043	35.287796
1228.628708	93159.883324	35.292813
1229.733419	93282.454877	35.297831
1231.018049	93432.113556	35.302848
1231.792986	93552.031951	35.307866
1233.553526	93675.165542	35.312884
1234.454354	93804.565471	35.317901
1235.589462	93968.906707	35.322919
1236.943574	94101.746740	35.327936
1237.757551	94226.836540	35.332954
1239.715899	94353.794486	35.337972
1240.732994	94486.304557	35.342989
1242.469802	94607.277533	35.348007
1243.555567	94777.287390	35.353024
1244.772389	94871.714829	35.358042
1245.779771	94994.905888	35.363060
1247.320508	95184.417297	35.368077
1247.942387	95298.486764	35.373095
1249.811917	95407.620664	35.378112
1250.501307	95596.163933	35.383130
1251.767261	95700.916715	35.388148
1253.363376	95881.417574	35.393165
1254.494283	95989.982237	35.398183
1255.732624	96167.537576	35.403200
1256.845853	96282.527074	35.408218
1258.162930	96456.390585	35.413236
1259.703260	96587.431907	35.418253
1260.689984	96757.567402	35.423271
1262.102555	96899.909916	35.428288
1263.747072	97012.844996	35.433306
1264.460812	97192.440194	35.438324
1265.829406	97350.183727	35.443341
1266.548747	97491.027016	35.448359
1267.599882	97639.681824	35.453376
1269.808092	97764.569695	35.458394
1270.868844	97967.301297	35.463412
1272.150145	98111.551184	35.468429
1273.561017	98237.511020	35.473447
1275.151818	98410.435039	35.478464
1276.254764	98538.805220	35.483482
1278.123478	98661.569392	35.488500
1279.638514	98846.769372	35.493517
1280.540405	98972.004389	35.498535
1282.422544	99081.324867	35.503552
1283.373334	99249.947389	35.508570
1284.864757	99414.157801	35.513588
1286.137308	99519.964771	35.518605
1287.307357	99657.466266	35.523623
1288.639265	99794.537947	35.528640
1289.820266	99938.973488	35.533658
1291.529473	100083.034944	35.538676
1292.404362	100197.392507	35.543693
1293.431790	100377.367813	35.548711
1294.464004	100463.559687	35.553728
1295.639612	100617.490721	35.558746
1296.717970	100723.435334	35.563764
1298.458603	100889.268015	35.568781
1299.152369	101009.207201	35.573799
1300.999088	101109.564872	35.578816
1302.214221	101260.583447	35.583834
1303.108099	101425.422008	35.588852
1304.582862	101525.600175	35.593869
1305.484523	101705.257810	35.598887
1306.839700	101815.415340	35.603904
1308.149871	101985.747069	35.608922
1309.300448	102122.165380	35.613940
1310.380724	102298.344462	35.618957
1311.752211	102443.227264	35.623975
1313.346365	102577.211267	35.628992
1314.103645	102741.403820	35.634010
1315.464654	102904.697963	35.639028
1316.953148	103071.478489	35.644045
1318.328101	103218.023384	35.649063
1319.239588	103402.128214	35.654080
1321.132637	103553.313336	35.659098
1322.136165	103703.729611	35.664116
1323.714771	103894.249898	35.669133
1324.951934	104041.922884	35.674151
1326.511904	104208.795051	35.679168
1327.991968	104368.150810	35.684186
1329.549392	104517.914735	35.689204
1331.176619	104652.848218	35.694221
1331.945221	104845.827331	35.699239
1333.780060	104983.476103	35.704256
1334.864084	105167.307842	35.709274
1336.270670	105292.825734	35.714292
1337.317929	105492.201623	35.719309
1339.022725	105624.786859	35.724327
1340.475157	105800.268535	35.729344
1341.901985	105926.754802	35.734362
1342.982748	106126.155994	35.739380
1344.373778	106267.964599	35.744397
1346.169035	106422.575685	35.749415
1347.399921	106604.851030	35.754432
1348.804457	106723.181214	35.759450
1350.161509	106912.862306	35.764468
1351.266862	107047.911317	35.769485
1352.616124	107234.596396	35.774503
1353.904285	107369.776385	35.779520
1355.591503	107510.171940	35.784538
1356.516782	107709.085732	35.789556
1357.926306	107847.850245	35.794573
1359.733641	107993.742006	35.799591
1360.973903	108184.293443	35.804608
1362.248960	108367.296646	35.809626
1363.425847	108506.082932	35.814644
1365.153023	108649.845847	35.819661
1366.436122	108839.288046	35.824679
1367.448192	108961.267587	35.829696
1369.567395	109068.451303	35.834714
1370.514141	109237.487722	35.839732
1372.151948	109407.320583	35.844749
1373.276301	109552.241646	35.849767
1374.300023	109698.717604	35.854784
1375.786563	109839.253523	35.859802
1376.949723	109986.050838	35.864820
1378.421074	110131.091096	35.869837
1379.787495	110286.060936	35.874855
1380.834080	110450.564286	35.879872
1382.291483	110587.735483	35.884890
1383.117812	110739.565923	35.889908
1384.787721	110865.349518	35.894925
1386.281864	111078.695456	35.899943
1387.587753	111261.177471	35.904960
1389.077516	111383.466662	35.909978
1390.419846	111558.418944	35.914996
1391.824687	111758.080822	35.920013
1393.345863	111914.517549	35.925031
1395.446894	112055.468592	35.930048
1396.886845	112200.785599	35.935066
1397.776481	112370.694587	35.940084
1399.060292	112576.921273	35.945101
1400.283382	112748.337069	35.950119
1401.510415	112893.381795	35.955136
1403.172971	113073.997420	35.960154
1404.477781	113228.698031	35.965172
1405.915790	113422.290973	35.970189
1407.573214	113598.397692	35.975207
1408.874267	113771.859192	35.980224
1410.857850	113946.992302	35.985242
1411.702515	114102.290548	35.990260
1413.877971	114286.878650	35.995277
1415.338635	114429.609856	36.000295
1416.469065	114621.013597	36.005312
1418.157890	114773.896504	36.010330
1419.716924	114935.353763	36.015348
1420.914495	115117.912939	36.020365
1422.605524	115252.078348	36.025383
1423.642818	115450.422755	36.030400
1425.405258	115585.977712	36.035418
1426.626471	115783.548466	36.040436
1428.443439	115913.905159	36.045453
1429.561779	116133.102567	36.050471
1430.400348	116284.230426	36.055488
1432.436361	116421.917946	36.060506
1433.644984	116594.736149	36.065524
1434.830892	116775.378137	36.070541
1436.210096	117002.309942	36.075559
1437.532528	117159.944270	36.080576
1439.589687	117302.286684	36.085594
1440.680359	117466.405000	36.090612
1442.073613	117685.768356	36.095629
1443.814461	117864.962293	36.100647
1445.072249	118024.119103	36.105664
1446.406221	118160.085098	36.110682
1447.970320	118297.091613	36.115700
1449.410245	118482.390640	36.120717
1450.734334	118609.882579	36.125735
1452.084546	118798.705859	36.130752
1453.370078	118937.621559	36.135770
1455.021271	119118.586031	36.140788
1456.442573	119256.715734	36.145805
1457.841824	119446.232453	36.150823
1459.209467	119602.576554	36.155840
1460.477107	119761.907153	36.160858
1461.763037	119972.777938	36.165876
1463.384123	120120.302462	36.170893
1464.996755	120295.525495	36.175911
1466.524326	120469.047227	36.180928
1467.946127	120644.385243	36.185946
1469.109113	120820.664724	36.190964
1470.788089	121023.623345	36.195981
1472.171360	121168.892993	36.200999
1474.065006	121343.185564	36.206016
1475.417494	121559.915963	36.211034
1476.634460	121712.712545	36.216052
1478.510256	121884.440601	36.221069
1479.652428	122090.557653	36.226087
1481.433742	122244.546823	36.231104
1483.303687	122453.109419	36.236122
1484.687548	122618.752505	36.241140
1486.138935	122811.502274	36.246157
1487.761513	122954.160039	36.251175
1489.187461	123175.603552	36.256192
1490.905957	123319.109294	36.261210
1492.394467	123541.787143	36.266228
1493.743701	123706.188624	36.271245
1495.125034	123871.510624	36.276263
1496.853239	124045.011361	36.281280
1498.530939	124250.490151	36.286298
1499.960367	124400.608623	36.291316
1501.175821	124590.748890	36.296333
1502.640113	124787.779399	36.301351
1504.248408	124940.646386	36.306368
1505.453980	125129.107419	36.311386
1507.162212	125348.573471	36.316404
1508.678171	125504.586958	36.321421
1510.436574	125694.547445	36.326439
1511.888739	125907.649402	36.331456
1513.226683	126064.099740	36.336474
1515.566773	126222.431153	36.341492
1516.655898	126430.832148	36.346509
1518.457487	126601.360977	36.351527
1519.996059	126760.481552	36.356544
1521.322030	126976.082049	36.361562
1522.909797	127163.521156	36.366580
1524.257012	127313.542214	36.371597
1526.381181	127461.819237	36.376615
1527.503352	127655.606090	36.381632
1529.167577	127830.129383	36.386650
1530.642848	127984.415447	36.391668
1531.804309	128111.301144	36.396685
1533.424695	128282.350643	36.401703
1534.527569	128479.465362	36.406720
1535.993058	128622.659449	36.411738
1536.890675	128787.682919	36.416756
1539.189395	128949.292433	36.421773
1540.442253	129127.968464	36.426791
1541.548126	129325.595482	36.431808
1543.552570	129479.197786	36.436826
1544.435457	129713.702738	36.441844
1545.913417	129886.495053	36.446861
1547.706689	130050.458970	36.451879
1549.248236	130222.977236	36.456896
1550.877062	130460.879239	36.461914
1552.163874	130674.399186	36.466932
1553.571197	130842.863207	36.471949
1555.164440	131022.650226	36.476967
1557.404866	131211.153354	36.481984
1558.930486	131424.717108	36.487002
1560.543957	131646.440284	36.492020
1562.094516	131812.366171	36.497037
1563.692599	131975.080096	36.502055
1565.225143	132190.663020	36.507072
1567.150462	132412.697442	36.512090
1568.484053	132624.995811	36.517108
1570.065236	132798.575207	36.522125
1572.329688	132954.803301	36.527143
1573.609994	133158.093108	36.532160
1575.252373	133373.490207	36.537178
1576.998481	133545.134778	36.542196
1578.212466	133768.445782	36.547213
1580.033331	133926.016706	36.552231
1581.606372	134153.670321	36.557248
1583.051688	134325.189971	36.562266
1585.177509	134503.470057	36.567284
1586.470973	134727.928950	36.572301
1588.485348	134889.275668	36.577319
1589.548840	135101.001806	36.582336
1591.323405	135286.843729	36.587354
1592.978794	135478.559820	36.592372
1594.626298	135678.540039	36.597389
1596.168395	135845.555108	36.602407
1597.671231	136049.159499	36.607424
1599.004178	136277.210144	36.612442
1600.803056	136433.860599	36.617460
1602.501593	136644.673509	36.622477
1604.077607	136814.983380	36.627495
1605.636266	137044.461425	36.632512
1607.751365	137215.410304	36.637530
1609.108686	137419.718989	36.642548
1610.878706	137601.724169	36.647565
1612.243441	137799.812368	36.652583
1614.437585	137962.098014	36.657600
1615.693878	138142.971610	36.662618
1617.378112	138310.700522	36.667636
1618.741958	138469.344483	36.672653
1620.571223	138643.603877	36.677671
1621.611003	138839.647043	36.682688
1623.361184	138971.417262	36.687706
1624.887494	139198.230645	36.692724
1625.671362	139357.529072	36.697741
1627.854936	139544.866479	36.702759
1628.812855	139741.701641	36.707776
1631.008668	139932.892115	36.712794
1632.291431	140145.202783	36.717812
1633.648073	140332.372310	36.722829
1635.838801	140523.960243	36.727847
1637.065832	140748.272935	36.732864
1638.946051	140925.084929	36.737882
1640.690155	141155.072274	36.742900
1642.033308	141344.848324	36.747917
1643.926979	141541.065085	36.752935
1645.027132	141761.248496	36.757952
1647.181004	141948.859114	36.762970
1648.374153	142208.573449	36.767988
1649.710229	142394.326880	36.773005
1652.319522	142603.681250	36.778023
1653.778395	142825.374323	36.783040
1655.376848	143036.463795	36.788058
1656.896010	143235.678740	36.793076
1658.655576	143469.914404	36.798093
1660.349610	143675.150165	36.803111
1662.152353	143914.718361	36.808128
1663.760803	144110.211126	36.813146
1665.969651	144293.758830	36.818164
1667.735603	144568.117678	36.823181
1669.818018	144741.839702	36.828199
1671.366235	144979.149728	36.833216
1672.384999	145173.627448	36.838234
1674.475952	145369.254355	36.843252
1676.463343	145569.322632	36.848269
1678.358093	145771.536376	36.853287
1679.977093	146031.975846	36.858304
1681.779458	146197.536734	36.863322
1683.977110	146394.813635	36.868340
1685.040629	146645.662196	36.873357
1686.968903	146802.244512	36.878375
1688.709276	147017.242710	36.883392
1690.229982	147251.963109	36.888410
1692.095952	147433.618961	36.893428
1693.087457	147635.569822	36.898445
1695.500647	147810.435252	36.903463
1697.009036	148056.508813	36.908480
1698.793292	148228.801709	36.913498
1700.462842	148440.360156	36.918516
1701.871072	148639.221542	36.923533
1703.908307	148862.424886	36.928551
1705.337040	149017.259353	36.933568
1706.796998	149228.374582	36.938586
1708.646391	149413.822059	36.943604
1710.050381	149593.205685	36.948621
1711.792670	149800.223220	36.953639
1713.666361	149957.032573	36.958656
1714.911495	150190.512594	36.963674
1716.640403	150362.711657	36.968692
1717.769488	150570.503388	36.973709
1720.006479	150754.426463	36.978727
1721.572751	150974.055449	36.983744
1723.031860	151205.987505	36.988762
1724.877121	151374.496965	36.993780
1726.764799	151614.617030	36.998797
1728.423650	151820.025271	37.003815
1730.424104	152004.728276	37.008832
1732.197653	152259.108460	37.013850
1733.873048	152445.146031	37.018868
1735.514123	152629.250349	37.023885
1737.449748	152888.161110	37.028903
1739.244446	153066.614345	37.033920
1741.112111	153305.139788	37.038938
1743.220439	153480.553363	37.043956
1744.901081	153696.708492	37.048973
1746.720135	153928.374365	37.053991
1748.799676	154119.631492	37.059008
1750.659104	154328.674946	37.064026
1752.580305	154542.806802	37.069044
1753.929637	154733.194421	37.074061
1755.663234	154965.502316	37.079079
1757.448899	155176.654809	37.084096
1759.026309	155375.187873	37.089114
1760.918380	155578.439548	37.094132
1762.420822	155814.936110	37.099149
1764.146241	156034.383141	37.104167
1766.148469	156240.233263	37.109184
1767.970523	156488.932178	37.114202
1769.675197	156672.921839	37.119220
1771.494407	156880.098214	37.124237
1773.235128	157120.610862	37.129255
1775.056688	157317.480821	37.134272
1776.713527	157533.144418	37.139290
1778.861689	157737.230564	37.144308
1780.704770	157993.456344	37.149325
1782.398690	158179.116898	37.154343
1784.392619	158407.298548	37.159360
1785.672719	158620.594138	37.164378
1787.825626	158800.352192	37.169396
1789.594115	159075.479003	37.174413
1791.279187	159278.455790	37.179431
1793.423100	159460.196861	37.184448
1795.162495	159713.129461	37.189466
1796.899534	159922.505531	37.194484
1798.949762	160121.599633	37.199501
1800.562259	160346.608217	37.204519
1801.620313	160539.128576	37.209536
1803.824523	160705.497084	37.214554
1805.581901	160932.033504	37.219572
1807.280905	161147.750822	37.224589
1808.778754	161326.306968	37.229607
1810.718791	161509.562031	37.234624
1812.838805	161708.780821	37.239642
1814.458469	161957.348030	37.244660
1816.279637	162143.326402	37.249677
1817.214189	162337.600817	37.254695
1818.862377	162557.316793	37.259712
1820.353957	162784.072045	37.264730
1823.347383	162996.589468	37.269748
1824.856992	163247.630703	37.274765
1826.636694	163433.356015	37.279783
1828.519727	163684.163458	37.284800
1830.384024	163875.876286	37.289818
1832.272866	164138.455075	37.294836
1834.127454	164327.584631	37.299853
1836.419940	164573.374398	37.304871
1837.988746	164768.499691	37.309888
1839.764465	165019.523601	37.314906
1841.872911	165222.124511	37.319924
1843.491936	165443.080120	37.324941
1845.539242	165698.060635	37.329959
1847.633932	165893.095745	37.334976
1849.845873	166102.368983	37.339994
1851.439762	166359.087500	37.345012
1853.584472	166551.124926	37.350029
1855.737531	166782.721049	37.355047
1857.680284	166967.943729	37.360064
1859.584692	167166.605110	37.365082
1861.925374	167422.667037	37.370100
1863.491846	167631.759598	37.375117
1865.272042	167829.378790	37.380135
1867.854027	168013.071936	37.385152
1868.920871	168223.616919	37.390170
1870.982197	168426.331534	37.395188
1872.624768	168674.915179	37.400205
1874.609472	168924.270608	37.405223
1876.332247	169125.926507	37.410240
1878.167915	169324.851157	37.415258
1880.768532	169519.215981	37.420276
1882.314075	169772.807065	37.425293
1883.957523	170022.160404	37.430311
1886.057167	170221.225397	37.435328
1887.473333	170417.571259	37.440346
1889.837166	170619.488441	37.445364
1891.700576	170838.787889	37.450381
1893.259574	171092.702635	37.455399
1895.335623	171271.240290	37.460416
1897.016993	171550.355875	37.465434
1899.030676	171739.636945	37.470452
1901.416413	171932.297511	37.475469
1902.682066	172187.407584	37.480487
1904.595169	172365.253058	37.485504
1906.567835	172548.544500	37.490522
1908.207579	172779.167446	37.495540
1909.786859	172977.834388	37.500557
1911.121960	173167.610590	37.505575
1914.012844	173348.692319	37.510592
1915.271411	173610.396437	37.515610
1916.912486	173836.699572	37.520628
1918.716228	174013.478854	37.525645
1920.818887	174255.453971	37.530663
1922.290147	174489.449913	37.535680
1924.538262	174686.928263	37.540698
1926.583608	174937.619073	37.545716
1928.766978	175134.539030	37.550733
1930.701317	175393.255137	37.555751
1933.023098	175587.440523	37.560768
1934.399053	175854.240434	37.565786
1936.898152	176048.247652	37.570804
1938.695284	176303.819765	37.575821
1941.011764	176514.337738	37.580839
1943.174714	176717.104352	37.585856
1944.828694	176934.364635	37.590874
1946.976172	177193.603854	37.595892
1948.947354	177416.195468	37.600909
1950.811557	177602.102507	37.605927
1952.955804	177864.530820	37.610944
1954.524524	178081.315875	37.615962
1956.708521	178308.471162	37.620980
1958.864828	178523.579411	37.625997
1960.580050	178769.537634	37.631015
1962.907521	178988.871292	37.636032
1965.172226	179194.006367	37.641050
1967.264708	179433.336635	37.646068
1969.323399	179647.489213	37.651085
1971.403206	179871.332716	37.656103
1973.517622	180083.182233	37.661120
1975.165506	180297.251030	37.666138
1977.365300	180529.604998	37.671156
1979.496756	180725.113357	37.676173
1981.616820	180983.923575	37.681191
1983.431021	181162.431934	37.686208
1985.577527	181366.987242	37.691226
1987.486470	181624.527966	37.696244
1989.210592	181820.943349	37.701261
1991.638010	182048.130776	37.706279
1993.486437	182269.473215	37.711296
1995.672072	182459.753340	37.716314
1997.231148	182701.927141	37.721332
1999.966312	182897.527186	37.726349
2001.397799	183131.717284	37.731367
2003.702614	183329.341550	37.736384
2005.824821	183566.888320	37.741402
2007.994258	183731.685346	37.746420
2009.907811	183988.363766	37.751437
2011.492230	184158.850887	37.756455
2013.750539	184379.973980	37.761472
2015.150566	184556.404833	37.766490
2017.605253	184731.844284	37.771508
2018.920030	184949.237114	37.776525
2021.036710	185134.629115	37.781543
2022.989354	185364.091463	37.786560
2024.837038	185536.914924	37.791578
2026.628601	185760.618636	37.796596
2028.348708	185949.020789	37.801613
2030.308489	186193.332564	37.806631
2032.499457	186384.580354	37.811648
2034.062804	186623.488247	37.816666
2036.340491	186835.141369	37.821684
2038.856272	187052.303005	37.826701
2040.785153	187292.704521	37.831719
2043.317303	187503.229061	37.836736
2045.294186	187710.797134	37.841754
2047.337836	187942.224928	37.846772
2049.290132	188142.997148	37.851789
2051.388147	188388.529589	37.856807
2053.913872	188589.212769	37.861824
2055.879971	188812.751390	37.866842
2057.851244	189051.505606	37.871860
2060.500514	189252.362388	37.876877
2062.382069	189474.191724	37.881895
2064.656772	189688.028359	37.886912
2066.437766	189906.855415	37.891930
2068.467120	190121.913128	37.896948
2070.753601	190344.189922	37.901965
2072.946667	190574.985169	37.906983
2075.416023	190790.204532	37.912000
2076.701309	191000.993334	37.917018
2079.171284	191242.750586	37.922036
2081.480180	191441.932012	37.927053
2083.406559	191674.069301	37.932071
2085.238645	191890.524156	37.937088
2087.285299	192123.989745	37.942106
2089.803824	192314.892463	37.947124
2091.876382	192550.894171	37.952141
2093.675599	192794.326551	37.957159
2096.242249	192984.653161	37.962176
2098.068200	193241.168011	37.967194
2100.343683	193428.052462	37.972212
2102.723076	193684.596051	37.977229
2104.445862	193881.101014	37.982247
2106.901084	194110.576935	37.987264
2109.286813	194347.755936	37.992282
2111.179919	194537.027747	37.997300
2113.925838	194752.372987	38.002317
2115.597099	195007.893470	38.007335
2117.325823	195196.914628	38.012352
2119.789934	195397.128139	38.017370
2121.756404	195621.053388	38.022388
2124.170000	195868.693132	38.027405
2125.842537	196046.595665	38.032423
2128.407327	196243.826658	38.037440
2129.938115	196456.782739	38.042458
2132.466271	196602.009359	38.047476
2134.186122	196825.979010	38.052493
2136.042147	197012.270614	38.057511
2138.341818	197212.060412	38.062528
2140.053093	197416.170801	38.067546
2142.156296	197619.445604	38.072564
2144.485695	197811.693814	38.077581
2146.389529	198056.442244	38.082599
2148.478379	198240.556321	38.087616
2150.194422	198482.455354	38.092634
2152.425968	198674.468403	38.097652
2154.534860	198937.262513	38.102669
2156.640359	199129.335286	38.107687
2158.871990	199385.486618	38.112704
2160.985451	199587.383899	38.117722
2163.219422	199845.085577	38.122740
2165.489181	200067.915642	38.127757
2167.329177	200294.749579	38.132775
2169.729489	200524.630759	38.137792
2171.839171	200785.428339	38.142810
2174.308197	200999.700964	38.147828
2176.498091	201250.485945	38.152845
2178.916593	201464.895345	38.157863
2180.790380	201734.188508	38.162880
2183.197882	201938.624649	38.167898
2185.398539	202162.756274	38.172916
2187.645711	202444.686997	38.177933
2189.891906	202687.079281	38.182951
2192.218382	202895.035190	38.187968
2194.657574	203115.896001	38.192986
2196.693028	203412.615064	38.198004
2199.140518	203609.828359	38.203021
2201.220098	203867.192578	38.208039
2203.702886	204100.071264	38.213056
2206.413415	204332.825935	38.218074
2207.997640	204567.753101	38.223092
2210.384693	204803.328247	38.228109
2212.568598	205038.619228	38.233127
2214.757253	205272.996451	38.238144
2217.025000	205504.632863	38.243162
2219.447202	205756.937097	38.248180
2221.879020	205968.594215	38.253197
2224.009221	206234.504179	38.258215
2226.418008	206471.225146	38.263232
2228.584261	206675.158048	38.268250
2230.318228	206945.132767	38.273268
2233.162415	207153.682127	38.278285
2235.127544	207399.769477	38.283303
2237.414762	207637.326839	38.288320
2239.573191	207844.057796	38.293338
2241.945449	208106.687980	38.298356
2244.619289	208320.295499	38.303373
2246.386172	208574.988001	38.308391
2248.696269	208770.095130	38.313408
2250.731119	208968.826461	38.318426
2252.999578	209177.943856	38.323444
2254.927906	209416.745744	38.328461
2256.603027	209600.835500	38.333479
2258.584795	209838.462621	38.338496
2261.015708	210055.732808	38.343514
2263.066342	210301.221697	38.348532
2265.548149	210501.918325	38.353549
2267.262896	210760.703277	38.358567
2269.346505	210990.638086	38.363584
2271.967171	211222.773730	38.368602
2273.887243	211478.266401	38.373620
2275.982329	211730.215741	38.378637
2278.218624	211975.046962	38.383655
2280.459271	212241.371828	38.388672
2282.775742	212500.627080	38.393690
2284.382019	212760.313365	38.398708
2287.082680	213046.119782	38.403725
2289.116557	213298.960976	38.408743
2291.352069	213603.887082	38.413760
2294.046664	213835.576102	38.418778
2296.059049	214141.085997	38.423796
2298.850923	214421.132749	38.428813
2301.010635	214674.225893	38.433831
2303.490272	214954.705274	38.438848
2305.425524	215253.973390	38.443866
2308.220955	215529.567919	38.448884
2310.489227	215800.333745	38.453901
2312.577653	216108.786056	38.458919
2315.055110	216364.882255	38.463936
2317.973055	216666.374995	38.468954
2320.241672	216949.346454	38.473972
2322.801441	217211.793625	38.478989
2325.325509	217486.664567	38.484007
2327.470354	217790.392366	38.489024
2330.264511	218031.894329	38.494042
2332.186995	218333.704454	38.499060
2334.695808	218586.490038	38.504077
2336.662792	218908.216579	38.509095
2339.533307	219141.508147	38.514112
2341.883472	219448.575115	38.519130
2344.287965	219714.522395	38.524148
2346.402071	219983.068756	38.529165
2348.629209	220290.412721	38.534183
2350.881464	220537.329027	38.539200
2353.666502	220849.513316	38.544218
2355.624848	221180.431206	38.549236
2358.427525	221467.919455	38.554253
2360.903359	221752.768814	38.559271
2362.845348	222031.990117	38.564288
2365.674850	222306.500741	38.569306
2367.714775	222587.029075	38.574324
2370.278744	222865.139050	38.579341
2372.623899	223135.183763	38.584359
2374.597299	223403.244055	38.589376
2377.022065	223654.384136	38.594394
2379.057499	223915.198778	38.599412
2381.404114	224162.086501	38.604429
2383.530809	224418.126750	38.609447
2385.630541	224693.256692	38.614464
2388.348610	224950.995290	38.619482
2390.800262	225234.731152	38.624500
2392.990171	225493.101210	38.629517
2395.154546	225776.503576	38.634535
2397.117759	226043.710919	38.639552
2399.770815	226349.208313	38.644570
2401.989103	226625.913262	38.649588
2404.555588	226907.503472	38.654605
2407.139772	227216.595819	38.659623
2409.087581	227506.184296	38.664640
2411.866990	227812.022569	38.669658
2414.137754	228101.815858	38.674676
2416.433246	228405.955215	38.679693
2418.793306	228708.967964	38.684711
2421.519419	229004.228572	38.689728
2424.112328	229304.996987	38.694746
2426.226690	229618.235930	38.699764
2428.611741	229917.337795	38.704781
2431.743051	230224.398636	38.709799
2433.793014	230542.501867	38.714816
2436.499305	230849.581414	38.719834
2438.830729	231159.769084	38.724852
2441.597079	231466.434838	38.729869
2444.048446	231765.278334	38.734887
2446.715178	232077.752521	38.739904
2449.610954	232373.175069	38.744922
2451.527676	232684.068506	38.749940
2454.279666	232989.217685	38.754957
2456.974795	233288.306771	38.759975
2459.450785	233600.816220	38.764992
2462.073466	233903.195030	38.770010
2464.702621	234201.459265	38.775028
2467.372947	234498.549569	38.780045
2469.674625	234812.893789	38.785063
2472.090668	235101.847970	38.790080
2475.186410	235400.803824	38.795098
2477.389464	235712.601257	38.800116
2479.937238	235996.178049	38.805133
2482.695345	236291.126265	38.810151
2484.722812	236589.086556	38.815168
2487.377955	236882.376459	38.820186
2489.621083	237185.561816	38.825204
2492.075963	237487.368346	38.830221
2494.541398	237790.723394	38.835239
2496.763525	238092.238328	38.840256
2499.813705	238394.384859	38.845274
2502.034783	238701.997435	38.850292
2504.655379	238987.043837	38.855309
2507.184525	239293.440880	38.860327
2509.206601	239567.738110	38.865344
2511.739060	239831.820761	38.870362
2514.097767	240110.917257	38.875380
2516.293411	240378.839073	38.880397
2518.985482	240673.962030	38.885415
2521.166470	240952.987129	38.890432
2523.917662	241221.711849	38.895450
2526.384486	241513.926249	38.900468
2528.590267	241804.252340	38.905485
2530.987821	242089.240164	38.910503
2533.427326	242398.097990	38.915520
2536.369134	242702.279599	38.920538
2538.580709	242999.694236	38.925556
2541.228567	243301.993488	38.930573
2543.924409	243601.568041	38.935591
2546.095500	243914.968001	38.940608
2548.921020	244223.540572	38.945626
2551.126734	244550.144773	38.950644
2553.681378	244859.269782	38.955661
2556.458475	245169.071484	38.960679
2558.863192	245486.451481	38.965696
2561.661662	245807.732341	38.970714
2564.211265	246135.428968	38.975732
2566.744167	246461.046158	38.980749
2569.164478	246800.042784	38.985767
2571.430404	247128.345510	38.990784
2574.236299	247450.035400	38.995802
2576.881770	247793.291477	39.000820
2579.477809	248135.997369	39.005837
2582.187348	248466.620542	39.010855
2584.495096	248808.078203	39.015872
2587.432753	249139.073133	39.020890
2590.269454	249477.679760	39.025908
2592.817315	249817.018722	39.030925
2595.849767	250140.151758	39.035943
2598.307503	250491.978532	39.040960
2600.870608	250812.215311	39.045978
2603.700078	251168.480723	39.050996
2606.143400	251496.180464	39.056013
2609.081971	251831.549891	39.061031
2611.484834	252167.639888	39.066048
2614.133594	252510.854878	39.071066
2616.513643	252858.558423	39.076084
2618.970129	253187.300757	39.081101
2622.084236	253535.651383	39.086119
2624.602449	253884.681314	39.091136
2627.355631	254208.729921	39.096154
2630.057774	254564.615918	39.101172
2632.580698	254898.634369	39.106189
2635.185572	255235.333033	39.111207
2638.103690	255577.113886	39.116224
2640.709908	255929.435836	39.121242
2643.248913	256260.024710	39.126260
2645.554449	256607.187980	39.131277
2648.373173	256943.169705	39.136295
2650.939730	257253.484699	39.141312
2653.635550	257570.384280	39.146330
2655.939548	257890.191447	39.151348
2658.180819	258198.298458	39.156365
2660.879989	258524.724761	39.161383
2663.505500	258851.036169	39.166400
2665.996221	259167.411560	39.171418
2668.432306	259511.053010	39.176436
2670.919593	259835.279201	39.181453
2673.866088	260168.425613	39.186471
2676.054471	260527.171445	39.191488
2679.037890	260862.649932	39.196506
2681.573337	261214.178129	39.201524
2683.872596	261566.938107	39.206541
2686.495825	261919.926635	39.211559
2689.051414	262296.144517	39.216576
2692.047937	262650.344925	39.221594
2694.928099	263016.020885	39.226612
2697.125964	263391.585465	39.231629
2700.078688	263749.960111	39.236647
2702.800024	264136.010253	39.241664
2705.768121	264496.288465	39.246682
2708.791959	264870.936337	39.251700
2711.144650	265255.979130	39.256717
2714.527671	265621.476549	39.261735
2717.258081	265996.756253	39.266752
2719.931320	266371.892929	39.271770
2722.500458	266744.252066	39.276788
2725.301801	267112.306997	39.281805
2728.572449	267484.911274	39.286823
2730.949835	267874.982305	39.291840
2733.498673	268255.322435	39.296858
2736.752051	268625.669380	39.301876
2739.192888	269003.588410	39.306893
2741.886356	269387.539053	39.311911
2744.476798	269773.309878	39.316928
2747.384558	270157.125418	39.321946
2750.547153	270536.810866	39.326964
2753.375651	270918.429256	39.331981
2756.553933	271295.826274	39.336999
2759.296343	271679.948156	39.342016
2762.206212	272051.087943	39.347034
2765.089840	272423.959441	39.352052
2767.559822	272809.826885	39.357069
2770.421666	273189.637178	39.362087
2773.004318	273564.360286	39.367104
2775.882494	273948.994807	39.372122
2778.488939	274329.099809	39.377140
2781.616751	274711.408608	39.382157
2784.418198	275085.690838	39.387175
2786.929697	275473.635237	39.392192
2789.792071	275848.314307	39.397210
2792.250077	276231.821583	39.402228
2795.007479	276628.186369	39.407245
2797.913000	277008.421901	39.412263
2800.887468	277352.446611	39.417280
2803.303083	277707.356215	39.422298
2805.959551	278061.313097	39.427316
2808.141478	278427.792712	39.432333
2811.179071	278781.587476	39.437351
2813.256616	279164.417808	39.442368
2815.861729	279532.100280	39.447386
2819.040400	279906.296685	39.452404
2821.319059	280301.034346	39.457421
2824.044619	280695.345425	39.462439
2826.394427	281086.235553	39.467456
2829.050157	281495.215008	39.472474
2832.064750	281900.885786	39.477492
2834.736034	282317.127630	39.482509
2837.835242	282731.142164	39.487527
2840.633522	283144.035500	39.492544
2843.221038	283560.518348	39.497562
2846.271470	283986.834820	39.502580
2848.797927	284415.952025	39.507597
2852.159711	284837.341039	39.512615
2854.889220	285271.734553	39.517632
2857.899431	285701.256595	39.522650
2860.810667	286144.486115	39.527668
2863.452411	286590.171088	39.532685
2866.687134	287018.258973	39.537703
2869.478850	287463.360280	39.542720
2872.147393	287920.648532	39.547738
2875.278751	288351.799493	39.552756
2878.134083	288802.782425	39.557773
2881.309125	289244.924706	39.562791
2884.421605	289694.392252	39.567808
2887.347507	290128.240540	39.572826
2890.400067	290573.626353	39.577844
2892.939621	291038.093866	39.582861
2896.139592	291478.704552	39.587879
2899.522947	291930.030756	39.592896
2902.273638	292364.589011	39.597914
2905.789703	292809.694387	39.602932
2908.106085	293258.621399	39.607949
2911.163755	293697.040612	39.612967
2914.403039	294139.494606	39.617984
2917.247943	294586.379344	39.623002
2920.466288	295033.889905	39.628020
2922.894926	295471.490657	39.633037
2926.071602	295925.407258	39.638055
2928.938046	296366.975729	39.643072
2932.042257	296827.658706	39.648090
2935.211717	297265.951124	39.653108
2937.918377	297711.479123	39.658125
2941.014044	298142.262209	39.663143
2944.116626	298590.849833	39.668160
2947.423475	299033.002763	39.673178
2950.504488	299472.573953	39.678196
2953.166480	299911.803917	39.683213
2956.007628	300330.683160	39.688231
2959.084127	300735.477083	39.693248
2961.704915	301138.513233	39.698266
2964.947613	301522.068713	39.703284
2967.603122	301928.399543	39.708301
2970.393468	302320.203881	39.713319
2973.438926	302727.486938	39.718336
2975.873059	303138.955228	39.723354
2978.793844	303548.770492	39.728372
2981.346718	303969.565242	39.733389
2984.407599	304395.206126	39.738407
2987.586818	304822.605063	39.743424
2989.841606	305255.787961	39.748442
2992.929801	305698.591434	39.753460
2995.453340	306143.616477	39.758477
2998.660642	306597.142576	39.763495
3001.569857	307058.486804	39.768512
3004.406110	307509.630038	39.773530
3007.602687	307966.607500	39.778548
3010.475877	308442.151149	39.783565
3013.700400	308905.242191	39.788583
3016.526464	309369.740743	39.793600
3019.240772	309841.468741	39.798618
3022.856033	310315.973258	39.803636
3025.698901	310792.909463	39.808653
3028.881296	311275.962054	39.813671
3032.030339	311755.182584	39.818688
3034.860708	312237.601024	39.823706
3038.430668	312719.417756	39.828724
3041.175465	313212.081357	39.833741
3044.648026	313683.902040	39.838759
3047.759484	314165.556336	39.843776
3050.652460	314658.901019	39.848794
3053.927519	315132.194240	39.853812
3057.309438	315615.348385	39.858829
3060.383306	316116.226233	39.863847
3063.545834	316590.013079	39.868864
3066.950214	317077.118798	39.873882
3069.951766	317555.117192	39.878900
3073.001575	318039.048698	39.883917
3076.009118	318509.447486	39.888935
3079.521256	318990.431090	39.893952
3082.432143	319479.075818	39.898970
3085.901862	319956.937290	39.903988
3088.867220	320433.453848	39.909005
3092.078392	320917.344959	39.914023
3094.951520	321394.099638	39.919040
3097.947056	321877.232390	39.924058
3101.267758	322359.701531	39.929076
3104.323073	322835.835480	39.934093
3107.645140	323318.375278	39.939111
3110.720814	323806.513113	39.944128
3113.859918	324291.412802	39.949146
3117.112531	324758.616171	39.954164
3120.042332	325253.168447	39.959181
3122.626610	325724.840176	39.964199
3125.809738	326167.311209	39.969216
3129.025922	326630.014676	39.974234
3131.892949	327057.776132	39.979252
3134.595513	327515.451290	39.984269
3137.475054	327966.442320	39.989287
3140.825855	328418.067239	39.994304
3143.589598	328878.619725	39.999322
3146.618737	329345.222127	40.004340
3149.455526	329815.026383	40.009357
3152.418889	330293.746421	40.014375
3155.491069	330768.179990	40.019392
3158.347877	331274.412239	40.024410
3161.913587	331765.495820	40.029428
3165.706855	332245.468539	40.034445
3168.716712	332740.848758	40.039463
3172.105247	333222.453359	40.044480
3174.882195	333737.416182	40.049498
3178.294262	334225.002949	40.054516
3181.423608	334716.617663	40.059533
3184.633901	335214.868879	40.064551
3187.683023	335728.580423	40.069568
3190.756353	336243.350717	40.074586
3194.127963	336725.796898	40.079604
3197.182538	337271.108621	40.084621
3200.158276	337790.503699	40.089639
3204.029458	338294.010471	40.094656
3207.069758	338834.360185	40.099674
3210.274982	339354.468217	40.104692
3213.392244	339875.652345	40.109709
3217.031587	340400.532780	40.114727
3220.398067	340928.828897	40.119744
3223.004076	341447.313367	40.124762
3226.721142	341972.142920	40.129780
3229.745986	342511.676461	40.134797
3233.108463	343047.191097	40.139815
3237.054140	343564.811010	40.144832
3239.943134	344107.957060	40.149850
3243.309480	344625.481708	40.154868
3246.413695	345165.816678	40.159885
3249.861466	345700.126115	40.164903
3253.297025	346224.226636	40.169920
3256.281632	346751.694129	40.174938
3259.849339	347282.237978	40.179956
3263.177689	347820.507069	40.184973
3266.421362	348351.066784	40.189991
3269.726268	348872.421796	40.195008
3273.208500	349411.336727	40.200026
3276.696236	349943.315088	40.205044
3279.695526	350482.651327	40.210061
3283.238915	351005.877766	40.215079
3286.623837	351536.562162	40.220096
3289.522125	352073.055346	40.225114
3292.796140	352610.143724	40.230132
3296.266783	353124.298522	40.235149
3299.597509	353662.331848	40.240167
3303.046396	354148.861713	40.245184
3306.036186	354638.302635	40.250202
3308.936816	355114.832675	40.255220
3311.863724	355610.645619	40.260237
3315.201571	356106.515671	40.265255
3318.277084	356605.849065	40.270272
3321.252396	357108.366201	40.275290
3324.289010	357621.046986	40.280308
3327.850846	358167.194756	40.285325
3331.050296	358669.406846	40.290343
3334.122409	359187.040636	40.295360
3336.930764	359740.980707	40.300378
3340.176122	360266.266182	40.305396
3343.470365	360812.401266	40.310413
3346.612897	361370.076884	40.315431
3350.106110	361921.979947	40.320448
3353.286233	362498.290833	40.325466
3356.707181	363068.313167	40.330484
3360.142280	363629.595802	40.335501
3363.158710	364217.002092	40.340519
3366.884469	364793.350506	40.345536
3370.170111	365375.572891	40.350554
3373.692862	365966.607256	40.355572
3377.129771	366546.582770	40.360589
3380.696118	367149.725235	40.365607
3384.294910	367732.121365	40.370624
3387.321994	368323.761213	40.375642
3390.932451	368925.197637	40.380660
3394.707314	369523.859175	40.385677
3397.946076	370122.977852	40.390695
3401.738661	370715.834442	40.395712
3405.092837	371323.748736	40.400730
3408.725723	371905.804333	40.405748
3412.261665	372505.527718	40.410765
3415.744770	373106.950952	40.415783
3419.526358	373693.424093	40.420800
3422.802481	374302.880815	40.425818
3426.459220	374894.177582	40.430836
3429.876812	375492.455675	40.435853
3432.960270	376109.071044	40.440871
3436.415652	376699.992882	40.445888
3440.302388	377297.713473	40.450906
3443.863279	377901.210478	40.455924
3447.581697	378497.366727	40.460941
3450.942408	379100.420481	40.465959
3454.570547	379670.340579	40.470976
3457.996341	380296.325279	40.475994
3461.681736	380891.638554	40.481012
3465.469144	381474.546681	40.486029
3468.390821	382070.622075	40.491047
3472.504171	382663.278090	40.496064
3475.731231	383262.508289	40.501082
3479.028827	383856.162476	40.506100
3483.062203	384447.357257	40.511117
3486.382435	385034.718477	40.516122
3489.856840	385551.611379	40.521127
3492.903670	386041.099868	40.526132
3495.751503	386478.125700	40.531136
3498.381681	386859.438658	40.536141
3500.559993	387216.025266	40.541146
3503.119192	387472.534598	40.546151
3505.044506	387701.577065	40.551156
3506.543327	387908.969086	40.556160
3508.479391	388063.830905	40.561165
3509.986440	388190.762701	40.566170
3511.509678	388260.425838	40.571175
3512.630076	388306.580040	40.576180
3513.277898	388315.148877	40.581184
3514.326564	388319.407747	40.586189
3514.879389	388294.857893	40.591194
3515.563302	388246.867359	40.596199
3515.902948	388175.434904	40.601204
3516.390113	388084.652999	40.606208
3516.632124	387983.458295	40.611213
3516.884449	387882.388824	40.616218
3517.147565	387751.107518	40.621223
3516.977553	387622.004830	40.626228
3517.222027	387495.023092	40.631232
3517.539878	387329.961418	40.636237
3517.134521	387174.320538	40.641242
3516.653370	387023.878631	40.646247
3516.950865	386868.862814	40.651252
3516.444793	386715.855170	40.656256
3516.589247	386554.530169	40.661261
3516.287748	386392.766348	40.666266
3516.332452	386242.060103	40.671271
3515.931849	386077.335224	40.676276
3515.599901	385922.643784	40.681280
3515.534838	385757.406691	40.686285
3515.114791	385601.354582	40.691290
3515.017558	385455.245081	40.696295
3514.810837	385306.787241	40.701300
3514.663054	385150.944509	40.706304
3514.356428	384994.439593	40.711309
3513.727001	384866.417100	40.716314
3513.908911	384713.241558	40.721319
3513.713321	384568.085079	40.726324
3513.287385	384442.394084	40.731328
3513.319178	384292.978974	40.736333
3512.808767	384138.384619	40.741338
3512.431493	384030.334121	40.746343
3512.195257	383895.099836	40.751348
3511.983491	383760.598723	40.756352
3511.837459	383667.642619	40.761357
3511.214684	383526.415298	40.766362
3510.677361	383426.475764	40.771367
3510.900101	383314.767870	40.776372
3510.461928	383212.675792	40.781376
3510.576178	383104.672109	40.786381
3510.126522	383028.802104	40.791386
3509.999392	382905.322234	40.796391
3509.828647	382820.201162	40.801396
3509.623740	382742.104697	40.806400
3509.529361	382642.093080	40.811405
3509.141138	382587.194429	40.816410
3509.311542	382469.719097	40.821415
3509.184242	382411.396388	40.826420
3509.040501	382314.977743	40.831424
3508.788108	382230.071721	40.836429
3508.707525	382185.398771	40.841434
3508.185070	382080.595649	40.846439
3508.129028	382040.954394	40.851444
3508.107767	381949.246016	40.856448
3508.337735	381875.097472	40.861453
3507.860434	381842.389557	40.866458
3507.768614	381743.545111	40.871463
3507.648357	381690.306843	40.876468
3507.574719	381638.892333	40.881472
3507.451143	381584.382776	40.886477
3507.222762	381516.028498	40.891482
3507.167213	381455.480285	40.896487
3507.130823	381420.718506	40.901492
3506.957337	381366.852368	40.906496
3507.195881	381302.391532	40.911501
3506.716839	381266.656809	40.916506
3506.603891	381215.578583	40.921511
3506.637308	381166.410112	40.926516
3506.567641	381127.253307	40.931520
3506.347827	381084.356009	40.936525
3505.872138	381042.287555	40.941530
3506.291665	381001.629007	40.946535
3505.713240	380969.673914	40.951540
3505.941351	380938.659524	40.956544
3506.240235	380903.742547	40.961549
3505.782644	380867.647990	40.966554
3505.979970	380815.858911	40.971559
3505.987039	380794.010107	40.976564
3506.017704	380757.202420	40.981568
3506.271478	380718.807961	40.986573
3506.031086	380678.736633	40.991578
3506.027525	380645.901950	40.996583
3505.749286	380614.662132	41.001588
3505.764659	380584.011728	41.006592
3505.752855	380549.804829	41.011597
3505.621119	380527.825211	41.016602
3505.380469	380495.078746	41.021607
3505.792708	380459.787374	41.026612
3505.826004	380430.965273	41.031616
3505.989368	380402.911049	41.036621
3505.793231	380365.096041	41.041626
3505.335098	380325.414846	41.046631
3505.639103	380299.118709	41.051636
3505.588844	380263.951137	41.056640
3505.919225	380227.934902	41.061645
3505.578282	380192.151923	41.066650
3505.290479	380174.774947	41.071655
3505.323831	380142.086610	41.076660
3505.365788	380119.672356	41.081664
3505.225852	380089.325891	41.086669
3505.149067	380058.435297	41.091674
3505.224730	380032.836369	41.096679
3504.983101	380033.078060	41.101684
3504.819506	379995.104943	41.106688
3505.055268	379969.506101	41.111693
3505.024600	379960.100229	41.116698
3504.751403	379931.936633	41.121703
3504.913453	379909.020021	41.126708
3504.936765	379875.163061	41.131712
3504.586657	379872.802148	41.136717
3504.886791	379831.576257	41.141722
3504.878338	379815.604732	41.146727
3504.822360	379799.182890	41.151732
3504.532258	379782.772616	41.156736
3504.961774	379764.773378	41.161741
3504.714220	379751.942639	41.166746
3504.739489	379718.899140	41.171751
3504.850274	379711.912570	41.176756
3504.714764	379684.312027	41.181760
3504.714277	379671.391337	41.186765
3504.782060	379675.373880	41.191770
3505.042630	379632.348175	41.196775
3504.603032	379609.323014	41.201780
3504.581318	379610.292985	41.206784
3505.050000	379563.826064	41.211789
3504.636589	379554.048205	41.216794
3504.904503	379534.548325	41.221799
3504.589008	379527.629105	41.226804
3504.709905	379515.401348	41.231808
3504.742047	379482.025913	41.236813
3504.560214	379475.467076	41.241818
3504.914459	379448.653732	41.246823
3504.629927	379432.623951	41.251828
3504.640868	379414.360066	41.256832
3504.720657	379405.190949	41.261837
3504.617356	379385.495325	41.266842
3504.740966	379364.746431	41.271847
3504.482354	379348.509040	41.276852
3504.271242	379320.157146	41.281856
3504.432085	379309.779756	41.286861
3504.003064	379295.934722	41.291866
3504.394023	379277.127440	41.296871
3504.571693	379262.677797	41.301876
3503.979525	379255.344434	41.306880
3504.384317	379237.628648	41.311885
3504.269781	379235.586546	41.316890
3504.099210	379226.456962	41.321895
3504.235313	379213.870620	41.326900
3504.280125	379203.511542	41.331904
3503.875399	379174.910364	41.336909
3503.984384	379181.989508	41.341914
3504.295077	379168.866854	41.346919
3504.259219	379162.284891	41.351924
3503.895964	379150.235292	41.356928
3503.944151	379134.763235	41.361933
3503.944631	379138.018857	41.366938
3504.088795	379123.930548	41.371943
3504.132350	379117.997334	41.376948
3504.234217	379113.809915	41.381952
3504.458401	379090.628654	41.386957
3504.057536	379094.609031	41.391962
3504.338830	379063.025176	41.396967
3504.282977	379059.015292	41.401972
3503.985377	379047.667464	41.406976
3504.401467	379032.366127	41.411981
3503.986744	379028.362098	41.416986
3504.235691	379011.764552	41.421991
3504.049556	379009.835497	41.426996
3503.912051	379001.641731	41.432000
3504.426246	378979.457399	41.437005
3503.795755	378963.405808	41.442010
3504.307166	378958.670369	41.447015
3504.270286	378956.158146	41.452020
3504.187786	378940.859282	41.457024
3504.481792	378925.297416	41.462029
3504.579657	378917.091862	41.467034
3504.607652	378895.671086	41.472039
3504.360622	378878.897533	41.477044
3504.348707	378876.991802	41.482048
3504.302005	378837.066016	41.487053
3504.131735	378855.202786	41.492058
3504.331551	378817.908704	41.497063
3504.250812	378811.282906	41.502068
3504.019696	378803.790646	41.507072
3504.047124	378798.979081	41.512077
3504.021911	378776.269457	41.517082
3504.183504	378762.865015	41.522087
3503.926276	378762.803956	41.527092
3503.821727	378748.780263	41.532096
3504.196657	378734.095763	41.537101
3503.973709	378737.539347	41.542106
3503.896665	378727.835287	41.547111
3504.143603	378716.172370	41.552116
3503.785241	378709.310652	41.557120
3504.345298	378690.094833	41.562125
3503.979930	378700.148664	41.567130
3504.295788	378669.118606	41.572135
3504.151426	378675.093301	41.577140
3504.002677	378669.444770	41.582144
3504.208063	378640.721326	41.587149
3504.160162	378650.496070	41.592154
3504.141429	378617.967309	41.597159
3504.166700	378623.355620	41.602164
3504.103077	378605.917077	41.607168
3503.988496	378605.833469	41.612173
3503.843665	378590.468016	41.617178
3503.990725	378573.250508	41.622183
3503.995630	378562.872136	41.627188
3503.742548	378562.199973	41.632192
3504.210836	378547.195422	41.637197
3504.208568	378526.262502	41.642202
3503.940135	378522.387909	41.647207
3504.281745	378515.975088	41.652212
3504.280212	378494.558763	41.657216
3504.318015	378479.698541	41.662221
3503.919126	378484.467163	41.667226
3503.904316	378449.775635	41.672231
3503.805993	378443.330603	41.677236
3503.721240	378470.509039	41.682240
3504.284220	378429.850583	41.687245
3503.857329	378441.135106	41.692250
3503.983732	378428.753530	41.697255
3503.900490	378407.019413	41.702260
3504.002569	378400.619002	41.707264
3504.277666	378392.283582	41.712269
3504.078814	378378.122052	41.717274
3504.314890	378363.383057	41.722279
3504.147024	378352.675844	41.727284
3503.973897	378345.530426	41.732288
3504.478181	378328.281781	41.737293
3503.892335	378323.974068	41.742298
3503.962835	378304.937190	41.747303
3504.145968	378289.138246	41.752308
3504.201167	378291.393302	41.757312
3504.352861	378281.017089	41.762317
3504.171744	378274.635987	41.767322
3503.896331	378250.464915	41.772327
3504.363248	378241.946529	41.777332
3503.958394	378229.292770	41.782336
3504.085872	378201.420698	41.787341
3503.648707	378198.030585	41.792346
3504.195213	378199.343175	41.797351
3504.281631	378183.279685	41.802356
3503.920972	378174.230776	41.807360
3504.400366	378151.847999	41.812365
3503.652634	378135.763732	41.817370
3503.852321	378141.506073	41.822375
3504.033600	378124.104912	41.827380
3503.604274	378120.179405	41.832384
3504.081468	378117.509561	41.837389
3503.729860	378105.457801	41.842394
3503.835321	378098.344609	41.847399
3504.030986	378100.730087	41.852404
3503.655048	378082.068900	41.857408
3503.823555	378069.527943	41.862413
3503.674554	378069.933052	41.867418
3503.895285	378072.772411	41.872423
3503.781829	378054.603869	41.877428
3503.895531	378054.535045	41.882432
3504.056609	378029.938742	41.887437
3503.532192	378029.589253	41.892442
3503.753195	378023.195418	41.897447
3503.987708	378016.494219	41.902452
3503.865778	377996.673669	41.907456
3504.033388	377994.943004	41.912461
3503.621866	378001.214387	41.917466
3503.715995	377981.029013	41.922471
3503.668124	377969.336170	41.927476
3503.838701	377969.410971	41.932480
3504.174387	377971.341916	41.937485
3503.852756	377953.562334	41.942490
3503.907161	377930.559847	41.947495
3503.888831	377944.043709	41.952500
3503.679416	377924.465874	41.957504
3503.832388	377911.520351	41.962509
3504.017463	377912.940956	41.967514
3503.646125	377887.309552	41.972519
3504.156227	377881.404147	41.977524
3503.700188	377893.380198	41.982528
3504.208320	377880.378524	41.987533
3503.805692	377865.613128	41.992538
3503.637732	377856.940659	41.997543
3503.634913	377858.263787	42.002548
3503.534475	377846.833576	42.007552
3503.998433	377829.565654	42.012557
3503.705998	377841.897396	42.017562
3503.449227	377843.667640	42.022567
3503.995678	377801.586751	42.027572
3503.256206	377828.436710	42.032576
3503.816912	377813.900555	42.037581
3503.750234	377814.953985	42.042586
3503.769220	377797.730951	42.047591
3503.936358	377794.194407	42.052596
3503.695258	377801.201957	42.057600
3503.918702	377779.139224	42.062605
3503.606477	377774.203174	42.067610
3503.419698	377766.322171	42.072615
3503.568910	377759.074823	42.077620
3503.331196	377781.114430	42.082624
3503.504999	377767.478800	42.087629
3503.135128	377755.378949	42.092634
3503.099112	377742.107143	42.097639
3503.292058	377745.459635	42.102644
3503.035657	377754.860584	42.107648
3503.619146	377760.618618	42.112653
3503.632693	377759.827987	42.117658
3503.434564	377760.953068	42.122663
3503.715153	377765.716112	42.127668
3503.685000	377759.311065	42.132672
3503.479486	377743.904005	42.137677
3503.681547	377744.787777	42.142682
3503.733933	377733.664043	42.147687
3503.842744	377730.925225	42.152692
3503.501852	377724.060574	42.157696
3503.826774	377725.916925	42.162701
3503.575152	377726.185643	42.167706
3503.121355	377708.935562	42.172711
3503.698618	377704.596540	42.177716
3503.494300	377711.318497	42.182720
3503.845108	377707.345938	42.187725
3503.859647	377699.382227	42.192730
3503.783501	377687.057875	42.197735
3503.629660	377687.234829	42.202740
3503.585534	377678.059464	42.207744
3503.827077	377675.197918	42.212749
3503.397524	377676.028917	42.217754
3503.585241	377655.803149	42.222759
3504.080257	377643.770037	42.227764
3503.633605	377649.716361	42.232768
3503.592341	377634.944629	42.237773
3503.587110	377641.813179	42.242778
3503.671115	377614.914134	42.247783
3503.753583	377627.517347	42.252788
3503.890769	377622.739162	42.257792
3503.806755	377602.174780	42.262797
3503.579268	377597.377929	42.267802
3503.655477	377610.643472	42.272807
3503.985915	377597.211948	42.277812
3503.804817	377585.133078	42.282816
3503.889582	377572.834126	42.287821
3503.756708	377566.445285	42.292826
3503.976346	377543.848868	42.297831
3504.141641	377542.474653	42.302836
3503.599990	377544.925842	42.307840
3503.811530	377516.327795	42.312845
3503.997079	377518.918395	42.317850
3503.480601	377523.553102	42.322855
3504.025968	377512.097020	42.327860
3503.693473	377497.549325	42.332864
3503.914450	377481.744079	42.337869
3503.851742	377483.712587	42.342874
3503.850875	377473.258535	42.347879
3503.867557	377474.019001	42.352884
3503.936726	377465.817683	42.357888
3504.079857	377438.171528	42.362893
3504.076717	377434.941666	42.367898
3503.723822	377418.540334	42.372903
3503.915206	377405.359651	42.377908
3503.874354	377405.086333	42.382912
3503.832848	377394.460632	42.387917
3503.629303	377391.822039	42.392922
3503.671679	377366.252084	42.397927
3503.723918	377371.102143	42.402932
3503.440463	377378.650620	42.407936
3503.505307	377356.841650	42.412941
3503.954572	377353.642013	42.417946
3503.745690	377355.938866	42.422951
3503.801634	377345.094259	42.427956
3503.518332	377332.878851	42.432960
3503.696327	377316.673356	42.437965
3503.598307	377326.151114	42.442970
3503.989746	377309.759260	42.447975
3503.899760	377291.942766	42.452980
3503.969599	377285.877943	42.457984
3503.882167	377283.093807	42.462989
3503.653091	377260.542724	42.467994
3503.660341	377258.583014	42.472999
3503.652599	377267.995642	42.478004
3503.575715	377264.980913	42.483008
3503.946102	377236.382993	42.488013
3503.643510	377239.534060	42.493018
3503.913396	377231.529893	42.498023
3503.822690	377217.325419	42.503028
3503.499890	377208.880774	42.508032
3503.700826	377203.278504	42.513037
3503.541439	377207.449822	42.518042
3503.814346	377192.348467	42.523047
3503.619118	377173.327618	42.528052
3503.759982	377165.496449	42.533056
3503.879045	377159.194900	42.538061
3503.295332	377166.154974	42.543066
3503.494679	377142.798451	42.548071
3503.780025	377136.572359	42.553076
3503.411886	377135.078961	42.558080
3503.552949	377138.287088	42.563085
3503.268770	377150.083576	42.568090
3503.414624	377142.251615	42.573095
3503.317022	377124.003834	42.578100
3503.162437	377120.899631	42.583104
3503.403120	377122.489527	42.588109
3503.434539	377134.312441	42.593114
3503.448126	377137.871390	42.598119
3503.885491	377127.500593	42.603124
3503.238210	377121.778028	42.608128
3503.593385	377108.037196	42.613133
3503.735290	377106.819281	42.618138
3503.728957	377103.386406	42.623143
3503.674950	377107.922621	42.628148
3503.106612	377089.698363	42.633152
3503.513107	377075.695044	42.638157
3503.411183	377081.637831	42.643162
3503.549131	377088.305790	42.648167
3503.743166	377084.968422	42.653172
3503.368572	377086.324907	42.658176
3503.733741	377065.002467	42.663181
3503.627329	377059.474196	42.668186
3503.605055	377056.883235	42.673191
3503.571976	377061.212656	42.678196
3503.312697	377054.182371	42.683200
3503.866716	377042.216061	42.688205
3503.641263	377036.859222	42.693210
3503.365367	377040.514811	42.698215
3503.665873	377041.561092	42.703220
3503.416190	377037.632517	42.708224
3503.601701	377016.338450	42.713229
3503.972287	377023.351190	42.718234
3503.811826	377007.097325	42.723239
3503.885519	377004.643810	42.728244
3503.504998	376990.408758	42.733248
3503.852485	376974.456133	42.738253
3503.455887	376983.319823	42.743258
3503.720170	376977.504017	42.748263
3503.874683	376946.472689	42.753268
3503.590613	376951.172470	42.758272
3503.889862	376950.972569	42.763277
3503.448869	376931.965019	42.768282
3503.582135	376918.004835	42.773287
3503.459544	376925.019241	42.778292
3503.315768	376930.739739	42.783296
3503.515532	376926.282253	42.788301
3503.635409	376928.196490	42.793306
3503.528572	376913.231366	42.798311
3503.797067	376904.184462	42.803316
3503.626558	376896.224406	42.808321
3503.649152	376893.066742	42.813325
3503.307917	376893.654867	42.818330
3503.675812	376872.611695	42.823335
3503.702792	376870.369046	42.828340
3503.516623	376879.835406	42.833345
3503.898665	376863.190492	42.838349
3503.670472	376848.753256	42.843354
3503.474285	376842.526926	42.848359
3503.726252	376845.921037	42.853364
3503.704806	376843.965843	42.858369
3503.586347	376825.187058	42.863373
3503.666044	376817.416364	42.868378
3503.621110	376804.425459	42.873383
3503.631015	376811.673305	42.878388
3503.366781	376815.301635	42.883393
3503.678794	376803.322636	42.888397
3503.459947	376786.696365	42.893402
3503.241117	376778.235195	42.898407
3503.434696	376786.929327	42.903412
3503.195660	376793.962163	42.908417
3503.567081	376783.957812	42.913421
3503.613611	376789.266701	42.918426
3503.453859	376771.308386	42.923431
3503.619040	376761.285758	42.928436
3503.212100	376766.920696	42.933441
3503.489281	376757.312783	42.938445
3503.616449	376763.931626	42.943450
3503.606069	376764.111343	42.948455
3503.587574	376750.124218	42.953460
3503.366338	376743.418539	42.958465
3503.530901	376733.701239	42.963469
3503.100860	376735.905905	42.968474
3503.391924	376743.694359	42.973479
3503.644381	376743.196617	42.978484
3503.260587	376733.922109	42.983489
3503.596546	376717.793149	42.988493
3503.812303	376723.126170	42.993498
3503.698891	376714.343084	42.998503
3503.762166	376712.552547	43.003508
3503.657291	376692.092743	43.008513
3503.768396	376681.468166	43.013517
3503.393419	376696.636762	43.018522
3503.436306	376682.894276	43.023527
3503.659669	376676.703347	43.028532
3503.559732	376675.854323	43.033537
3503.869834	376655.430650	43.038541
3503.813909	376655.312328	43.043546
3503.473051	376654.068966	43.048551
3503.663660	376631.349442	43.053556
3503.360819	376637.400365	43.058561
3503.562669	376629.152467	43.063565
3503.460192	376630.262460	43.068570
3503.651675	376622.601240	43.073575
3503.563283	376608.040073	43.078580
3503.474280	376612.047707	43.083585
3503.492638	376605.227822	43.088589
3503.612173	376611.440911	43.093594
3503.729482	376600.866206	43.098599
3503.661591	376596.196626	43.103604
3503.668632	376581.951040	43.108609
3503.901470	376571.485247	43.113613
3503.281889	376579.239626	43.118618
3503.565693	376566.527355	43.123623
3503.622372	376555.199123	43.128628
3503.413321	376555.232190	43.133633
3503.417037	376551.695933	43.138637
3503.662561	376566.741057	43.143642
3503.370620	376547.455397	43.148647
3503.474794	376522.129503	43.153652
3503.423955	376519.975446	43.158657
3503.789236	376521.164122	43.163661
3503.618959	376521.674355	43.168666
3503.677203	376523.725538	43.173671
3503.730395	376494.999176	43.178676
3503.348198	376485.826105	43.183681
3503.458925	376485.223580	43.188685
3503.643592	376490.408926	43.193690
3503.975629	376484.633212	43.198695
3503.836661	376471.097457	43.203700
3503.307412	376469.883868	43.208705
3503.595906	376460.146913	43.213709
3503.314766	376467.339080	43.218714
3503.323572	376452.940550	43.223719
3503.301874	376443.176313	43.228724
3503.286095	376442.085051	43.233729
3502.860650	376427.246421	43.238733
3503.027954	376439.836596	43.243738
3503.373538	376443.775551	43.248743
3503.338481	376447.952730	43.253748
3503.216860	376437.746427	43.258753
3503.287306	376438.320357	43.263757
3503.142065	376460.753056	43.268762
3503.319031	376449.253160	43.273767
3503.609413	376443.585772	43.278772
3503.353602	376454.614878	43.283777
3503.568458	376424.769135	43.288781
3503.140707	376427.914612	43.293786
3503.446224	376422.626379	43.298791
3503.186898	376420.708767	43.303796
3503.124356	376425.577084	43.308801
3503.284573	376427.484969	43.313805
3503.518624	376433.451053	43.318810
3503.274336	376428.911084	43.323815
3503.539552	376433.651281	43.328820
3503.648095	376425.647022	43.333825
3503.458130	376411.254460	43.338829
3503.676337	376410.355140	43.343834
3503.673015	376404.250876	43.348839
3503.855439	376376.292540	43.353844
3503.626526	376390.039142	43.358849
3503.649267	376362.716519	43.363853
3503.384821	376376.748546	43.368858
3503.007916	376372.789142	43.373863
3503.180556	376369.734902	43.378868
3503.552181	376383.361141	43.383873
3503.737640	376359.624810	43.388877
3503.087968	376353.749892	43.393882
3503.061730	376346.453714	43.398887
3503.546085	376349.938317	43.403892
3503.518635	376345.109695	43.408897
3503.293257	376338.379166	43.413901
3503.438228	376352.677162	43.418906
3503.427142	376337.544069	43.423911
3503.868179	376314.047116	43.428916
3503.680184	376325.650582	43.433921
3503.685631	376313.821646	43.438925
3503.729378	376306.336341	43.443930
3503.920114	376292.875593	43.448935
3503.801246	376286.687828	43.453940
3503.689448	376288.689591	43.458945
3503.734994	376267.137449	43.463949
3503.475453	376262.396378	43.468954
3503.351962	376258.803894	43.473959
3503.424426	376261.361578	43.478964
3503.562860	376259.101277	43.483969
3503.742666	376245.820299	43.488973
3503.317797	376234.517223	43.493978
3503.350620	376231.612259	43.498983
3503.607883	376225.721144	43.503988
3503.525564	376224.640394	43.508993
3503.798584	376218.187178	43.513997
3503.633868	376209.641023	43.519002
3503.601350	376201.150281	43.524007
3503.551573	376188.566932	43.529012
3503.397126	376201.004547	43.534017
3503.381798	376194.189918	43.539021
3503.472454	376192.496777	43.544026
3503.404461	376185.461539	43.549031
3503.517803	376181.526368	43.554036
3503.324168	376185.296215	43.559041
3503.448658	376180.850546	43.564045
3503.411169	376185.562311	43.569050
3503.588642	376186.526315	43.574055
3503.481276	376154.721796	43.579060
3503.347800	376159.957474	43.584065
3503.545594	376148.403327	43.589069
3503.510230	376153.674371	43.594074
3503.486027	376148.336475	43.599079
3503.666030	376135.386109	43.604084
3503.496057	376129.766010	43.609089
3503.305456	376127.048976	43.614093
3503.529940	376122.307688	43.619098
3503.493776	376130.682162	43.624103
3503.186617	376119.335010	43.629108
3503.541516	376128.690581	43.634113
3503.726731	376095.873165	43.639117
3503.558105	376095.772657	43.644122
3503.551901	376090.253849	43.649127
3503.740315	376094.802731	43.654132
3503.168928	376088.762778	43.659137
3503.439622	376070.710672	43.664141
3503.582030	376068.729539	43.669146
3503.379424	376067.820421	43.674151
3503.335879	376067.216839	43.679156
3503.177290	376071.439022	43.684161
3503.744669	376066.948768	43.689165
3503.212133	376059.376453	43.694170
3503.309180	376046.108491	43.699175
3503.589144	376032.913359	43.704180
3503.462568	376044.074769	43.709185
3503.569621	376037.698633	43.714189
3503.451404	376047.536000	43.719194
3503.342503	376035.699621	43.724199
3503.547123	376025.772324	43.729204
3503.547552	376018.395561	43.734209
3503.750032	376010.452682	43.739213
3503.463929	376013.194246	43.744218
3503.168855	376008.738569	43.749223
3503.677188	376013.694754	43.754228
3503.504305	375994.211952	43.759233
3503.379130	375983.090365	43.764237
3503.368850	375980.599188	43.769242
3503.495846	375979.917773	43.774247
3503.619764	375982.009475	43.779252
3503.147159	375978.141471	43.784257
3503.360041	375966.406828	43.789261
3503.739083	375961.234098	43.794266
3503.502985	375953.106165	43.799271
3503.801968	375944.486656	43.804276
3503.473529	375952.780182	43.809281
3503.187006	375937.258050	43.814285
3503.356301	375923.520762	43.819290
3503.053620	375919.880261	43.824295
3503.743872	375922.009630	43.829300
3503.455968	375917.400187	43.834305
3503.753543	375915.954133	43.839309
3503.645111	375919.786847	43.844314
3503.287399	375897.458832	43.849319
3503.629033	375883.439917	43.854324
3503.621372	375885.170868	43.859329
3503.762630	375886.191479	43.864333
3503.800082	375890.764247	43.869338
3503.730413	375874.928005	43.874343
3503.329144	375861.891375	43.879348
3503.109006	375855.414308	43.884353
3503.251101	375858.317129	43.889357
3503.078695	375867.094750	43.894362
3503.381404	375861.018339	43.899367
3503.281120	375860.067605	43.904372
3503.204699	375865.803043	43.909377
3503.406586	375859.386451	43.914381
3503.222338	375843.263064	43.919386
3503.631988	375832.667384	43.924391
3503.364131	375830.445847	43.929396
3503.172719	375827.067557	43.934401
3503.504197	375833.476197	43.939405
3503.351318	375845.430369	43.944410
3503.060217	375846.926318	43.949415
3503.513921	375840.775162	43.954420
3503.307664	375830.276840	43.959425
3503.603643	375812.347809	43.964429
3503.488870	375811.297615	43.969434
3503.058061	375805.845888	43.974439
3503.347350	375818.213477	43.979444
3503.228331	375826.117807	43.984449
3503.512414	375811.090482	43.989453
3503.320507	375801.531056	43.994458
3503.154161	375814.988154	43.999463
3503.604151	375790.522874	44.004468
3503.249279	375777.122764	44.009473
3503.139723	375774.469207	44.014477
3503.299017	375780.294582	44.019482
3503.403220	375788.316256	44.024487
3503.863710	375790.787196	44.029492
3503.382419	375781.807688	44.034497
3503.407169	375755.222015	44.039501
3503.553845	375762.524741	44.044506
3503.362972	375763.368922	44.049511
3503.297452	375760.148786	44.054516
3503.461983	375755.518681	44.059521
3503.050974	375752.200535	44.064525
3503.351519	375760.114866	44.069530
3503.300037	375765.235886	44.074535
3503.747902	375756.592803	44.079540
3503.226472	375744.796112	44.084545
3503.469391	375736.694164	44.089549
3503.479743	375738.854705	44.094554
3503.264678	375746.112867	44.099559
3503.525644	375746.580379	44.104564
3503.564764	375744.844492	44.109569
3503.671443	375723.282398	44.114573
3503.565048	375709.537742	44.119578
3503.422395	375708.517390	44.124583
3503.553242	375714.601643	44.129588
3503.276957	375725.150877	44.134593
3503.132632	375706.502848	44.139597
3503.128450	375685.950307	44.144602
3502.865651	375689.298701	44.149607
3503.135082	375692.690149	44.154612
3503.519917	375697.640459	44.159617
3503.210108	375687.158468	44.164621
3503.307257	375684.446794	44.169626
3503.274458	375694.652301	44.174631
3503.762377	375686.435304	44.179636
3503.368966	375694.255847	44.184641
3503.620797	375689.662809	44.189645
3503.332019	375667.476393	44.194650
3502.959841	375652.578184	44.199655
3503.085590	375654.415242	44.204660
3503.042646	375664.240803	44.209665
3503.186046	375646.895436	44.214669
3503.087517	375671.635971	44.219674
3503.207560	375668.259310	44.224679
3503.844687	375666.454327	44.229684
3503.323030	375670.123450	44.234689
3503.397196	375658.130837	44.239693
3503.659209	375661.421712	44.244698
3503.104989	375658.355130	44.249703
3503.171800	375638.605333	44.254708
3503.281770	375647.338365	44.259713
3503.473728	375640.846996	44.264717
3503.286962	375647.439335	44.269722
3503.249042	375646.504175	44.274727
3503.604346	375652.095087	44.279732
3503.270563	375658.405417	44.284737
3503.304462	375656.390543	44.289741
3503.321131	375648.349779	44.294746
3503.239138	375634.804738	44.299751
3503.275026	375620.325320	44.304756
3503.265549	375627.957999	44.309761
3503.538174	375617.689170	44.314765
3503.362678	375628.629493	44.319770
3503.271811	375627.270269	44.324775
3503.616691	375620.932785	44.329780
3503.182178	375631.176371	44.334785
3503.516274	375622.907365	44.339789
3503.385215	375597.389144	44.344794
3502.979760	375602.667886	44.349799
3503.140541	375599.310217	44.354804
3503.057277	375597.771729	44.359809
3502.986206	375599.182032	44.364813
3502.961961	375603.357589	44.369818
3503.063781	375601.128478	44.374823
3503.336056	375596.430449	44.379828
3503.443471	375609.666280	44.384833
3503.459748	375600.328270	44.389837
3503.411271	375606.568072	44.394842
3503.305350	375616.047479	44.399847
3503.658842	375602.331840	44.404852
3503.459598	375587.508020	44.409857
3503.576970	375577.467220	44.414861
3503.667301	375582.565845	44.419866
3503.428563	375579.067830	44.424871
3503.574806	375559.305438	44.429876
3503.415675	375570.650185	44.434881
3503.578261	375538.726200	44.439885
3503.604713	375549.253062	44.444890
3503.268401	375553.096395	44.449895
3503.552635	375554.221600	44.454900
3503.384042	375551.551923	44.459905
3503.946997	375524.779275	44.464909
3503.667743	375503.914003	44.469914
3503.169354	375524.622432	44.474919
3503.658985	375505.619727	44.479924
3503.743304	375500.925961	44.484929
3503.804348	375482.983047	44.489933
3503.252437	375485.868412	44.494938
3503.362514	375479.949582	44.499943
3503.494650	375476.520119	44.504948
3503.162438	375489.901794	44.509953
3503.709466	375475.290652	44.514957
3503.662930	375457.797167	44.519962
3503.242482	375455.548855	44.524967
3503.372988	375452.068772	44.529972
3503.358632	375438.741911	44.534977
3503.254323	375445.779119	44.539981
3503.310130	375454.673378	44.544986
3503.653910	375448.743038	44.549991
3503.346298	375421.700939	44.554996
3503.170877	375423.076868	44.560001
3503.403078	375410.423268	44.565005
3503.323849	375412.852360	44.570010
3503.367979	375424.317641	44.575015
3503.302513	375420.385225	44.580020
3503.484448	375425.927262	44.585025
3503.582581	375417.313954	44.590029
3503.361342	375400.534868	44.595034
3503.133799	375386.376819	44.600039
3503.531374	375383.363261	44.605044
3503.054150	375389.645432	44.610049
3502.867966	375396.619280	44.615053
3503.425286	375387.831631	44.620058
3503.235656	375392.465788	44.625063
3503.596119	375392.129019	44.630068
3503.315641	375400.211577	44.635073
3503.343463	375393.542616	44.640077
3503.158257	375376.350826	44.645082
3503.096991	375371.094999	44.650087
3503.381261	375360.824265	44.655092
3503.037554	375377.133091	44.660097
3503.677186	375362.710769	44.665101
3503.608412	375363.790031	44.670106
3503.450203	375371.217333	44.675111
3503.508140	375363.653300	44.680116
3503.368083	375354.289072	44.685121
3503.290491	375344.787781	44.690125
3503.333323	375339.947930	44.695130
3503.053378	375328.952379	44.700135
3503.189135	375334.527165	44.705140
3503.238934	375351.893043	44.710145
3502.952569	375338.024086	44.715149
3503.255275	375335.101833	44.720154
3503.070667	375353.547697	44.725159
3503.268815	375346.495681	44.730164
3503.660300	375343.890081	44.735169
3503.739309	375339.680446	44.740173
3503.609613	375333.519685	44.745178
3503.762573	375324.999441	44.750183
3503.629389	375315.303431	44.755188
3503.527419	375320.686861	44.760193
3503.676925	375308.580487	44.765197
3503.764706	375298.010110	44.770202
3503.692733	375286.294863	44.775207
3503.547591	375289.675566	44.780212
3503.192276	375286.399452	44.785217
3503.203638	375259.306824	44.790221
3503.290001	375260.336128	44.795226
3503.134627	375264.100012	44.800231
3503.512949	375259.385181	44.805236
3503.612150	375261.124704	44.810241
3503.433748	375257.566248	44.815245
3503.262431	375259.653782	44.820250
3503.408853	375256.629041	44.825255
3503.477207	375256.592820	44.830260
3503.275874	375238.004463	44.835265
3503.357153	375227.206159	44.840269
3503.445833	375224.724729	44.845274
3503.096101	375222.439788	44.850279
3503.400881	375225.825688	44.855284
3503.148716	375233.852928	44.860289
3502.870156	375235.881103	44.865293
3503.385926	375226.413177	44.870298
3503.304026	375246.750662	44.875303
3503.318809	375239.676738	44.880308
3503.297153	375228.589456	44.885313
3503.448644	375212.845185	44.890317
3503.102348	375209.135202	44.895322
3502.753816	375209.444692	44.900327
3503.436892	375209.209549	44.905332
3503.328689	375205.767180	44.910337
3503.121514	375206.741136	44.915341
3503.412357	375212.342299	44.920346
3503.288762	375209.538299	44.925351
3503.334691	375215.127301	44.930356
3503.076111	375222.163497	44.935361
3503.253255	375222.364454	44.940365
3503.111760	375217.070414	44.945370
3502.626113	375227.296746	44.950375
3503.017370	375218.102875	44.955380
3503.099845	375223.762411	44.960385
3503.318458	375224.134874	44.965389
3503.408539	375234.651760	44.970394
3503.321337	375218.919784	44.975399
3503.470951	375194.679692	44.980404
3503.365828	375187.828213	44.985409
3503.260866	375190.185073	44.990413
3503.390306	375197.770437	44.995418
3503.110879	375197.331316	45.000423
3503.702491	375190.140765	45.005428
3503.339453	375201.085410	45.010433
3503.451509	375187.127984	45.015437
3503.430313	375171.563619	45.020442
3503.134814	375163.343168	45.025447
3503.294769	375164.386279	45.030452
3503.196206	375162.087069	45.035457
3503.249882	375160.348856	45.040461
3503.260064	375168.436389	45.045466
3503.024139	375175.799699	45.050471
3503.374851	375165.035101	45.055476
3503.186126	375176.486385	45.060481
3503.265032	375175.583621	45.065485
3503.336794	375178.573922	45.070490
3503.172460	375165.041741	45.075495
3503.511312	375143.264578	45.080500
3503.581727	375148.926031	45.085505
3503.385753	375135.449717	45.090509
3503.153025	375144.898403	45.095514
3503.111699	375145.973331	45.100519
3503.147187	375120.759173	45.105524
3503.357485	375142.551334	45.110529
3503.399513	375152.160086	45.115533
3503.434864	375130.303705	45.120538
3503.266089	375116.568710	45.125543
3503.793210	375103.766647	45.130548
3503.157412	375106.487235	45.135553
3503.507690	375101.420695	45.140557
3503.870019	375103.296693	45.145562
3503.561717	375088.642556	45.150567
3503.602609	375077.290971	45.155572
3503.618025	375067.367913	45.160577
3503.781107	375079.424989	45.165581
3503.631479	375057.470621	45.170586
3503.412633	375046.516211	45.175591
3503.455045	375050.503225	45.180596
3503.139413	375043.176246	45.185601
3503.161452	375038.339647	45.190605
3503.488749	375037.219553	45.195610
3503.494859	375042.026308	45.200615
3503.680887	375031.287708	45.205620
3503.488628	375022.262344	45.210625
3503.641071	375003.185519	45.215629
3503.708372	374998.443510	45.220634
3503.722720	375002.740215	45.225639
3503.787035	374991.181403	45.230644
3503.315046	374979.452987	45.235649
3503.600016	374976.940515	45.240653
3503.346505	374971.257148	45.245658
3503.277846	374975.312602	45.250663
3503.376368	374973.669043	45.255668
3503.207661	374976.214055	45.260673
3503.353421	374959.071524	45.265677
3503.325443	374948.112354	45.270682
3503.181241	374939.359189	45.275687
3503.372169	374935.055508	45.280692
3503.360394	374943.019368	45.285697
3503.099077	374943.493136	45.290701
3503.526360	374943.349302	45.295706
3503.117000	374950.765505	45.300711
3503.433990	374943.211320	45.305716
3503.513922	374945.793344	45.310721
3503.444528	374923.241156	45.315725
3503.304136	374914.385633	45.320730
3503.082791	374912.258443	45.325735
3503.338043	374913.820687	45.330740
3503.191408	374919.465607	45.335745
3503.043946	374918.802121	45.340749
3503.142787	374908.484273	45.345754
3503.151401	374922.728012	45.350759
3503.142315	374923.467161	45.355764
3502.925582	374928.843346	45.360769
3503.003031	374921.327021	45.365773
3502.986186	374928.782933	45.370778
3502.702967	374930.939047	45.375783
3503.121244	374915.457741	45.380788
3503.128837	374919.908150	45.385793
3503.128553	374925.580809	45.390797
3503.039409	374931.064013	45.395802
3503.045369	374930.427151	45.400807
3503.072324	374921.290800	45.405812
3503.143855	374932.192260	45.410817
3503.042467	374932.284621	45.415821
3502.819916	374928.834866	45.420826
3503.009060	374944.245629	45.425831
3503.092736	374941.154471	45.430836
3503.175925	374946.991996	45.435841
3503.283367	374939.394621	45.440845
3503.408687	374940.621276	45.445850
3503.450929	374939.826054	45.450855
3503.674387	374934.118161	45.455860
3503.286471	374922.274688	45.460865
3503.411625	374909.892232	45.465869
3503.441554	374909.480520	45.470874
3503.339727	374913.388597	45.475879
3503.540440	374903.080081	45.480884
3503.355279	374908.502153	45.485889
3503.318971	374905.124706	45.490893
3503.476955	374896.552704	45.495898
3503.389070	374883.746037	45.500903
3503.126634	374890.325021	45.505908
3503.354772	374894.537069	45.510913
3503.012874	374889.834293	45.515917
3503.493105	374895.151186	45.520922
3503.092334	374907.195692	45.525927
3503.776532	374895.182739	45.530932
3503.186395	374887.314058	45.535937
3503.118749	374867.152703	45.540941
3503.379490	374855.359302	45.545946
3503.227631	374850.015977	45.550951
3503.623068	374856.541850	45.555956
3503.086017	374867.157962	45.560961
3503.343156	374853.889745	45.565965
3503.709876	374866.754137	45.570970
3503.482171	374865.441956	45.575975
3503.686145	374838.852794	45.580980
3502.896107	374842.157411	45.585985
3503.136468	374836.039829	45.590989
3503.325215	374829.370777	45.595994
3503.351801	374837.175967	45.600999
3503.415403	374844.339363	45.606004
3503.378448	374843.200530	45.611009
3503.306251	374843.797030	45.616013
3503.434149	374842.377761	45.621018
3503.049759	374825.191788	45.626023
3503.176568	374803.371651	45.631028
3502.945719	374804.934426	45.636033
3503.010629	374807.595146	45.641037
3503.291072	374808.161342	45.646042
3503.211001	374804.307488	45.651047
3503.501889	374799.759053	45.656052
3503.124751	374812.537545	45.661057
3503.045868	374807.513369	45.666061
3503.245465	374808.346721	45.671066
3502.846858	374812.072782	45.676071
3503.041679	374807.539532	45.681076
3503.280786	374813.403305	45.686081
3503.420746	374806.309520	45.691085
3503.310126	374819.758136	45.696090
3503.145807	374828.254885	45.701095
3503.477283	374815.763474	45.706100
3503.139212	374819.123836	45.711105
3503.210833	374817.916964	45.716109
3503.330648	374789.051681	45.721114
3503.120311	374798.598657	45.726119
3503.126047	374785.700848	45.731124
3502.820955	374787.606050	45.736129
3503.144625	374783.790124	45.741133
3503.387281	374788.686706	45.746138
3503.304111	374788.267433	45.751143
3503.374083	374781.998714	45.756148
3503.237405	374799.648680	45.761153
3503.359262	374798.561055	45.766157
3503.639754	374785.823316	45.771162
3503.493401	374785.999098	45.776167
3503.710991	374763.350583	45.781172
3503.708118	374762.867741	45.786177
3503.301538	374750.950856	45.791181
3503.512754	374753.079698	45.796186
3503.376066	374758.773942	45.801191
3503.585528	374737.729274	45.806196
3503.277377	374739.227958	45.811201
3503.289514	374732.383305	45.816205
3503.528429	374723.416907	45.821210
3503.361193	374721.840784	45.826215
3503.482435	374731.767805	45.831220
3503.233122	374730.433597	45.836225
3503.330317	374728.281482	45.841229
3503.226524	374708.074887	45.846234
3503.183029	374696.685661	45.851239
3503.329541	374697.934412	45.856244
3503.475698	374692.162391	45.861249
3503.414404	374672.457817	45.866253
3503.325011	374694.068649	45.871258
3503.293349	374700.662060	45.876263
3503.565778	374684.389713	45.881268
3503.604855	374689.649179	45.886273
3503.512518	374670.356515	45.891277
3503.548853	374650.789124	45.896282
3503.458655	374649.048194	45.901287
3503.681798	374662.087973	45.906292
3503.351529	374668.118084	45.911297
3502.807919	374619.999385	45.916301
3503.245675	374650.608214	45.921306
3502.750431	374636.314157	45.926311
3503.395697	374630.361481	45.931316
3503.057886	374632.068359	45.936321
3503.212462	374639.370037	45.941325
3503.122309	374627.479411	45.946330
3502.883292	374640.159809	45.951335
3503.190567	374646.063706	45.956340
3503.446717	374620.432793	45.961345
3503.335053	374627.903747	45.966349
3503.528570	374651.810161	45.971354
3503.227316	374624.588465	45.976359
3503.365723	374656.389312	45.981364
3503.417699	374630.765242	45.986369
3503.165061	374642.659220	45.991373
3503.116323	374612.752068	45.996378
3502.906781	374614.794801	46.001383
3503.240939	374617.769102	46.006388
3502.684386	374621.392958	46.011393
3503.125119	374630.480926	46.016397
3503.370198	374609.023558	46.021402
3503.044317	374629.196413	46.026407
3503.045834	374612.610732	46.031412
3503.040865	374631.053962	46.036417
3503.359814	374610.449803	46.041421
3503.110418	374609.242793	46.046426
3503.115305	374648.034718	46.051431
3503.405803	374601.234101	46.056436
3503.371307	374638.582303	46.061441
3503.452655	374632.718767	46.066445
3503.638955	374629.128045	46.071450
3503.394312	374625.758070	46.076455
3503.632178	374600.740542	46.081460
3503.200240	374608.974386	46.086465
3503.620770	374595.120626	46.091469
3503.548575	374592.562837	46.096474
3503.410449	374596.654747	46.101479
3503.880624	374584.446594	46.106484
3503.343421	374576.391421	46.111489
3503.547121	374567.227053	46.116493
3503.737546	374563.686549	46.121498
3503.543260	374557.103437	46.126503
3503.432090	374551.855393	46.131508
3503.337451	374522.820320	46.136513
3503.234863	374517.799856	46.141517
3503.396466	374513.195512	46.146522
3503.100873	374525.910326	46.151527
3503.338827	374521.548293	46.156532
3503.267241	374525.629691	46.161537
3503.247727	374531.458072	46.166541
3503.377050	374533.548995	46.171546
3503.309176	374534.526384	46.176551
3503.366830	374516.049388	46.181556
3503.407535	374499.940788	46.186561
3503.426295	374498.182629	46.191565
3503.678068	374489.265023	46.196570
3503.319672	374489.398011	46.201575
3503.229534	374499.536566	46.206580
3503.379965	374499.258429	46.211585
3503.296354	374489.427199	46.216589
3503.564813	374464.048622	46.221594
3503.496717	374460.320032	46.226599
3503.213225	374444.618788	46.231604
3503.318014	374468.132327	46.236609
3503.372215	374456.778467	46.241613
3503.090585	374452.116990	46.246618
3502.628863	374472.718401	46.251623
3503.092078	374466.641851	46.256628
3503.273816	374463.662346	46.261633
3503.106382	374467.428208	46.266637
3503.416096	374469.007298	46.271642
3503.161372	374465.791531	46.276647
3503.117503	374471.979901	46.281652
3503.352578	374481.431105	46.286657
3503.268186	374463.332670	46.291661
3503.725875	374449.879993	46.296666
3503.262599	374455.193460	46.301671
3503.221139	374448.280918	46.306676
3503.462474	374451.397094	46.311681
3503.405642	374458.325215	46.316685
3503.151355	374462.639003	46.321690
3503.121873	374460.888468	46.326695
3503.363486	374445.943671	46.331700
3502.824270	374440.941341	46.336705
3502.935711	374461.935476	46.341709
3503.226059	374463.873759	46.346714
3503.502556	374459.709130	46.351719
3503.285106	374432.779315	46.356724
3503.306110	374433.920724	46.361729
3503.252571	374421.998813	46.366733
3503.520330	374418.471509	46.371738
3503.084578	374435.634710	46.376743
3503.538362	374416.128410	46.381748
3503.393419	374422.358202	46.386753
3503.300711	374425.679811	46.391757
3503.504128	374403.084214	46.396762
3503.181044	374395.707422	46.401767
3503.211207	374389.902819	46.406772
3502.762680	374393.662245	46.411777
3503.035401	374394.585799	46.416781
3503.123505	374391.086892	46.421786
3503.205304	374390.209092	46.426791
3503.236817	374389.288365	46.431796
3503.289918	374389.051051	46.436801
3503.034880	374396.392083	46.441805
3503.671942	374380.189168	46.446810
3503.093152	374404.904631	46.451815
3503.328755	374385.203863	46.456820
3503.273052	374400.500907	46.461825
3503.200656	374398.248394	46.466829
3503.617114	374389.304734	46.471834
3502.914767	374366.852294	46.476839
3503.351892	374351.164294	46.481844
3502.988799	374374.166772	46.486849
3503.072384	374364.283645	46.491853
3503.274752	374363.437662	46.496858
3503.112055	374365.065994	46.501863
3503.407989	374362.322809	46.506868
3503.108131	374373.308562	46.511873
3503.281891	374369.185602	46.516877
3503.599065	374361.351464	46.521882
3503.177036	374375.994159	46.526887
3503.529226	374365.508937	46.531892
3503.290179	374344.840222	46.536897
3503.240050	374340.981592	46.541901
3503.596949	374338.483150	46.546906
3503.513609	374343.990952	46.551911
3503.445674	374333.088810	46.556916
3503.342889	374335.928697	46.561921
3503.390728	374339.253535	46.566925
3503.249145	374315.822095	46.571930
3503.072584	374305.064307	46.576935
3503.236210	374296.135156	46.581940
3503.088116	374309.030225	46.586945
3502.818689	374311.082439	46.591949
3503.412054	374305.010731	46.596954
3503.098915	374309.028582	46.601959
3503.327589	374301.717182	46.606964
3503.498351	374309.067236	46.611969
3503.211504	374306.009162	46.616973
3503.719363	374311.677896	46.621978
3502.809508	374325.787209	46.626983
3503.336053	374311.331521	46.631988
3503.489728	374313.698424	46.636993
3502.927190	374300.559598	46.641997
3503.141971	374282.795363	46.647002
3503.333968	374274.980995	46.652007
3502.943547	374292.137090	46.657012
3503.061934	374290.007041	46.662017
3503.151901	374283.684209	46.667021
3503.258489	374274.229870	46.672026
3503.109575	374293.408270	46.677031
3503.242285	374280.286727	46.682036
3503.116963	374282.621419	46.687041
3502.928399	374284.381034	46.692045
3503.292001	374281.805214	46.697050
3503.098600	374288.373381	46.702055
3503.084019	374279.167139	46.707060
3503.043917	374284.057602	46.712065
3502.890143	374295.478168	46.717069
3503.149051	374283.939273	46.722074
3502.764128	374297.177040	46.727079
3503.144336	374288.340841	46.732084
3502.898827	374298.885575	46.737089
3502.784755	374303.075464	46.742093
3503.120251	374302.132121	46.747098
3503.321423	374303.728376	46.752103
3503.357384	374293.547503	46.757108
3503.226031	374308.169713	46.762113
3503.340573	374303.674536	46.767117
3503.699600	374306.772119	46.772122
3503.270918	374307.552168	46.777127
3503.445742	374287.326763	46.782132
3503.349932	374270.145817	46.787137
3503.350702	374272.333388	46.792141
3503.195397	374262.131866	46.797146
3503.273001	374280.842018	46.802151
3503.473701	374261.731783	46.807156
3503.313190	374265.089561	46.812161
3503.479871	374278.621710	46.817165
3503.661896	374261.345966	46.822170
3503.036143	374251.371434	46.827175
3503.270471	374236.122456	46.832180
3503.506204	374241.427207	46.837185
3503.309112	374234.055908	46.842189
3503.624036	374229.630801	46.847194
3503.259216	374233.198943	46.852199
3503.290134	374226.249485	46.857204
3503.005913	374231.814494	46.862209
3502.932776	374233.835684	46.867213
3503.201985	374232.521247	46.872218
3503.199149	374214.969449	46.877223
3503.196544	374205.888488	46.882228
3503.381436	374201.280428	46.887233
3503.019529	374201.693790	46.892237
3503.231130	374208.910216	46.897242
3503.154648	374210.957373	46.902247
3503.444515	374196.615372	46.907252
3503.005962	374214.872944	46.912257
3502.965008	374212.233879	46.917261
3503.342049	374201.897316	46.922266
3503.316213	374216.044993	46.927271
3503.247251	374218.040085	46.932276
3503.482693	374213.703855	46.937281
3503.399538	374208.222396	46.942285
3503.466659	374178.550996	46.947290
3503.156373	374183.916627	46.952295
3503.146580	374172.496491	46.957300
3503.200374	374173.098523	46.962305
3503.289955	374183.742947	46.967309
3503.302447	374173.209621	46.972314
3503.147970	374182.544405	46.977319
3503.043830	374181.136354	46.982324
3503.357189	374182.231556	46.987329
3503.238725	374189.296655	46.992333
3503.327005	374186.789789	46.997338
3502.937141	374191.760989	47.002343
3503.297118	374189.007669	47.007348
3503.313769	374189.183125	47.012353
3503.263539	374174.767686	47.017357
3503.511218	374160.712161	47.022362
3503.006315	374159.163955	47.027367
3503.215656	374149.642469	47.032372
3503.158149	374168.933667	47.037377
3503.028601	374154.988646	47.042381
3503.406897	374151.571038	47.047386
3503.183904	374163.282401	47.052391
3503.354671	374164.323829	47.057396
3503.470001	374156.114548	47.062401
3502.953477	374167.134605	47.067405
3503.391472	374163.987379	47.072410
3502.994617	374164.431705	47.077415
3503.181899	374171.321286	47.082420
3503.321073	374164.787153	47.087425
3503.000520	374140.976895	47.092429
3503.296184	374130.449672	47.097434
3503.205221	374128.607089	47.102439
3503.312070	374128.208649	47.107444
3503.394566	374135.725314	47.112449
3503.315352	374141.283368	47.117453
3503.374207	374130.437445	47.122458
3503.106780	374134.498963	47.127463
3503.182792	374136.089571	47.132468
3503.221194	374143.002691	47.137473
3503.042807	374134.381949	47.142477
3503.163875	374134.490023	47.147482
3503.103659	374137.094251	47.152487
3503.254368	374129.464450	47.157492
3503.371714	374128.911721	47.162497
3503.113686	374119.362355	47.167501
3503.440169	374104.353142	47.172506
3503.108910	374101.174883	47.177511
3503.183924	374108.056783	47.182516
3503.347054	374109.328362	47.187521
3503.639853	374113.225011	47.192525
3503.281741	374099.697673	47.197530
3502.650348	374114.653375	47.202535
3503.227554	374104.081642	47.207540
3503.079962	374102.985715	47.212545
3503.341278	374119.301153	47.217549
3503.374801	374105.254022	47.222554
3503.520518	374095.106628	47.227559
3503.418932	374075.967777	47.232564
3503.106163	374079.425952	47.237569
3503.202671	374075.162545	47.242573
3503.099766	374081.334867	47.247578
3503.227874	374072.665664	47.252583
3503.345689	374068.882213	47.257588
3503.273655	374067.341893	47.262593
3503.057527	374071.802319	47.267597
3503.087363	374078.462422	47.272602
3503.112123	374080.213762	47.277607
3503.379017	374079.255821	47.282612
3503.215242	374083.148331	47.287617
3503.099803	374074.288682	47.292621
3503.416403	374062.282720	47.297626
3503.154065	374052.962963	47.302631
3503.100495	374046.128582	47.307636
3503.184479	374055.171319	47.312641
3503.002874	374053.317622	47.317645
3503.095081	374048.011927	47.322650
3503.162505	374055.683619	47.327655
3503.124872	374048.643215	47.332660
3503.351001	374052.117959	47.337665
3503.635371	374052.403725	47.342669
3503.606294	374044.369879	47.347674
3503.502542	374055.604536	47.352679
3503.484742	374044.974214	47.357684
3503.326810	374037.494936	47.362689
3503.067183	374030.998384	47.367693
3503.322238	374018.366182	47.372698
3503.482370	374020.401385	47.377703
3503.291997	374026.791047	47.382708
3503.204140	374028.433000	47.387713
3503.275992	374027.505889	47.392717
3503.172668	374028.641523	47.397722
3503.218401	374028.227304	47.402727
3503.319888	374015.161490	47.407732
3503.031317	374005.896745	47.412737
3502.802001	374004.508476	47.417741
3502.876392	374007.294940	47.422746
3503.115181	374029.388445	47.427751
3503.596016	374017.407385	47.432756
3502.971321	374003.311638	47.437761
3502.867441	374000.250057	47.442765
3503.290993	373995.044608	47.447770
3502.950320	373991.638884	47.452775
3503.126049	373997.131218	47.457780
3503.255092	374001.537090	47.462785
3503.153165	374008.116279	47.467789
3503.229352	374005.662190	47.472794
3503.572686	374012.374501	47.477799
3503.306122	374011.348254	47.482804
3503.052662	374013.779532	47.487809
3502.803420	373998.479715	47.492813
3503.134621	374005.931653	47.497818
3503.296668	374018.294462	47.502823
3503.391178	374006.349028	47.507828
3503.296229	374014.326215	47.512833
3503.109830	374018.476689	47.517837
3503.129228	374026.461236	47.522842
3502.998220	374014.729521	47.527847
3503.359256	374004.700697	47.532852
3503.214876	373992.436886	47.537857
3503.055385	373984.169261	47.542861
3503.364256	373981.983648	47.547866
3503.376998	373984.932488	47.552871
3503.505648	373985.522690	47.557876
3503.590834	373985.814504	47.562881
3503.110789	373988.815803	47.567885
3503.530692	373984.730210	47.572890
3503.330872	373972.042708	47.577895
3503.233214	373944.432245	47.582900
3503.272990	373944.222473	47.587905
3502.978800	373956.072340	47.592909
3503.191606	373937.519684	47.597914
3503.026884	373954.818308	47.602919
3503.333863	373938.489331	47.607924
3503.490916	373943.297792	47.612929
3503.026121	373949.654531	47.617933
3503.243285	373961.041991	47.622938
3503.471816	373955.205971	47.627943
3503.211995	373945.224397	47.632948
3503.164720	373945.231891	47.637953
3502.797736	373962.791429	47.642957
3503.101819	373954.628586	47.647962
3503.317702	373957.876014	47.652967
3503.402344	373954.581124	47.657972
3503.258315	373928.555152	47.662977
3503.216950	373925.280177	47.667981
3503.310647	373918.346182	47.672986
3503.200447	373920.449560	47.677991
3503.370804	373917.700759	47.682996
3503.088959	373918.406727	47.688001
3503.156660	373924.399475	47.693005
3503.375580	373918.005326	47.698010
3503.082207	373934.917283	47.703015
3503.545096	373938.787062	47.708020
3503.408661	373930.235961	47.713025
3502.871937	373915.159624	47.718029
3502.980241	373902.474271	47.723034
3503.134457	373922.291758	47.728039
3503.405587	373914.286746	47.733044
3503.183127	373888.018764	47.738049
3503.111616	373901.436058	47.743053
3503.243165	373882.514648	47.748058
3503.248312	373886.889239	47.753063
3503.246668	373883.913242	47.758068
3503.183315	373896.311717	47.763073
3503.188631	373892.240774	47.768077
3503.478638	373892.805472	47.773082
3503.012657	373905.369342	47.778087
3503.319733	373900.233169	47.783092
3503.312545	373898.097512	47.788097
3503.123876	373900.645746	47.793101
3503.256049	373888.338189	47.798106
3503.584047	373878.594378	47.803111
3503.325523	373868.536266	47.808116
3503.382520	373864.915041	47.813121
3503.178109	373871.154316	47.818125
3503.702880	373842.376988	47.823130
3503.027159	373875.350098	47.828135
3503.587325	373847.126821	47.833140
3503.435484	373860.658580	47.838145
3503.197446	373846.654289	47.843149
3503.598711	373827.334082	47.848154
3503.225439	373828.588709	47.853159
3503.316628	373839.945239	47.858164
3503.055504	373838.867252	47.863169
3503.166181	373840.859404	47.868173
3503.345422	373818.979583	47.873178
3503.071378	373838.737615	47.878183
3503.154627	373837.554315	47.883188
3502.965860	373845.291981	47.888193
3502.837196	373841.979923	47.893197
3503.307103	373829.542647	47.898202
3503.554195	373827.086970	47.903207
3503.493421	373831.166727	47.908212
3503.377899	373806.051951	47.913217
3503.227162	373799.639903	47.918221
3503.557489	373803.378019	47.923226
3503.451904	373801.639486	47.928231
3503.343364	373796.187424	47.933236
3503.212645	373810.479010	47.938241
3503.674406	373794.634275	47.943245
3503.204880	373769.728066	47.948250
3503.321763	373776.806910	47.953255
3503.409523	373777.607085	47.958260
3503.140676	373780.040808	47.963265
3503.190850	373771.638245	47.968269
3503.407457	373770.637369	47.973274
3503.097239	373784.092434	47.978279
3503.343513	373768.383506	47.983284
3503.185845	373780.033774	47.988289
3503.469511	373765.005769	47.993293
3503.115751	373739.216338	47.998298
3503.378751	373738.487950	48.003303
3503.095770	373734.615194	48.008308
3503.094258	373745.299568	48.013313
3502.958296	373738.554477	48.018317
3503.487989	373720.587591	48.023322
3503.336819	373738.774507	48.028327
3503.009513	373744.727967	48.033332
3503.601596	373738.707256	48.038337
3503.174843	373745.388711	48.043341
3503.207329	373740.473993	48.048346
3503.193076	373732.030728	48.053351
3503.325453	373743.355336	48.058356
3503.388408	373733.856895	48.063361
3503.463413	373709.882109	48.068365
3503.510068	373697.359068	48.073370
3503.212551	373698.499969	48.078375
3503.301867	373692.533288	48.083380
3503.545690	373699.439448	48.088385
3503.125456	373695.613824	48.093389
3503.258860	373702.232177	48.098394
3503.135037	373712.376250	48.103399
3503.336789	373689.780527	48.108404
3503.401065	373673.871387	48.113409
3503.151454	373678.031887	48.118413
3503.143234	373662.337709	48.123418
3502.949467	373666.311313	48.128423
3503.175697	373672.151846	48.133428
3503.214948	373654.465966	48.138433
3503.054277	373656.806281	48.143437
3503.091761	373677.710750	48.148442
3503.148860	373668.264097	48.153447
3503.168435	373658.340042	48.158452
3503.048114	373664.438864	48.163457
3502.980678	373669.791612	48.168461
3503.388334	373671.660512	48.173466
3503.172494	373680.725286	48.178471
3503.146669	373674.064527	48.183476
3503.166251	373679.250888	48.188481
3503.187313	373679.044073	48.193485
3503.245593	373688.599720	48.198490
3503.270755	373679.030925	48.203495
3503.593807	373656.619518	48.208500
3503.114296	373651.251515	48.213505
3503.042061	373652.534876	48.218509
3503.297929	373643.082235	48.223514
3503.138635	373635.145208	48.228519
3503.235599	373635.231656	48.233524
3503.121698	373644.204008	48.238529
3503.065665	373645.510246	48.243533
3503.295656	373653.843153	48.248538
3503.029175	373647.652884	48.253543
3503.802001	373651.295629	48.258548
3503.316110	373647.404063	48.263553
3503.116650	373649.292618	48.268557
3503.156011	373624.509387	48.273562
3503.005957	373629.035731	48.278567
3503.020227	373621.478281	48.283572
3503.099340	373616.479862	48.288577
3503.191391	373612.039043	48.293581
3503.214974	373621.244053	48.298586
3503.153887	373619.498478	48.303591
3503.184854	373609.954188	48.308596
3503.139906	373610.215699	48.313601
3503.226947	373617.146656	48.318605
3503.230876	373600.687381	48.323610
3503.237082	373614.168799	48.328615
3503.137502	373626.013435	48.333620
3503.432799	373621.082598	48.338625
3503.113501	373631.283028	48.343629
3503.360736	373621.679116	48.348634
3503.051046	373624.882457	48.353639
3503.189969	373621.248260	48.358644
3503.320173	373620.744369	48.363649
3503.125314	373626.371648	48.368653
3503.350205	373587.618803	48.373658
3503.396650	373582.345721	48.378663
3503.244505	373583.107508	48.383668
3503.289823	373585.211758	48.388673
3503.249229	373588.957649	48.393677
3503.307416	373578.493265	48.398682
3502.940755	373586.742431	48.403687
3503.353975	373584.591179	48.408692
3503.239659	373587.890832	48.413697
3503.137784	373596.912170	48.418701
3503.261958	373592.313641	48.423706
3503.312738	373598.741564	48.428711
3503.067732	373587.104063	48.433716
3503.211387	373568.740243	48.438721
3503.057289	373586.953126	48.443725
3503.044607	373577.390289	48.448730
3502.891944	373581.459159	48.453735
3503.202855	373569.250446	48.458740
3503.255403	373564.179904	48.463745
3503.351760	373568.336604	48.468749
3503.265085	373572.598550	48.473754
3503.119104	373574.733040	48.478759
3503.402828	373569.066311	48.483764
3503.527518	373572.506253	48.488769
3503.258597	373570.640899	48.493773
3503.357798	373583.090087	48.498778
3503.088707	373584.633514	48.503783
3503.247033	373571.762083	48.508788
3503.227683	373540.170572	48.513793
3502.598898	373561.256736	48.518797
3502.863133	373543.535244	48.523802
3503.133633	373594.445763	48.528807
3502.815269	373588.111057	48.533812
3503.144908	373579.028317	48.538817
3502.894899	373612.773810	48.543821
3503.192061	373588.636644	48.548826
3503.284186	373588.494911	48.553831
3503.156796	373570.021305	48.558836
3503.121732	373569.797923	48.563841
3502.861722	373558.213662	48.568845
3503.074322	373575.885253	48.573850
3503.190627	373579.428275	48.578855
3503.074015	373558.485429	48.583860
3503.275949	373565.856126	48.588865
3502.922864	373562.986537	48.593869
3503.257720	373552.300342	48.598874
3503.063692	373563.600280	48.603879
3503.166543	373550.356034	48.608884
3503.546482	373569.018716	48.613889
3503.163375	373549.262723	48.618893
3503.583450	373546.805124	48.623898
3503.266286	373564.484146	48.628903
3503.666289	373550.226267	48.633908
3503.669392	373538.167955	48.638913
3503.183896	373524.228110	48.643917
3503.263861	373507.858534	48.648922
3503.262905	373522.740230	48.653927
3503.213326	373516.159517	48.658932
3503.599027	373522.941526	48.663937
3503.113689	373515.691978	48.668941
3503.281070	373526.273395	48.673946
3503.034967	373530.789494	48.678951
3502.862184	373538.880830	48.683956
3502.913547	373531.826270	48.688961
3502.896749	373534.169288	48.693965
3503.712483	373525.721975	48.698970
3503.472911	373520.341466	48.703975
3503.365884	373506.926875	48.708980
3503.531829	373499.523496	48.713985
3503.280210	373494.755412	48.718989
3503.436369	373493.357069	48.723994
3502.888013	373492.756931	48.728999
3503.284817	373492.795982	48.734004
3503.412237	373504.070562	48.739009
3502.992377	373509.758862	48.744013
3503.223848	373485.606582	48.749018
3502.993519	373500.244721	48.754023
3503.144294	373500.704241	48.759028
3503.511208	373503.190114	48.764033
3503.175204	373487.038914	48.769037
3503.326122	373458.930942	48.774042
3502.981427	373468.550340	48.779047
3503.073279	373469.451629	48.784052
3503.283099	373460.464119	48.789057
3502.951697	373464.434061	48.794061
3503.265525	373456.625720	48.799066
3503.359882	373469.482725	48.804071
3503.144697	373466.845715	48.809076
3503.236161	373455.104113	48.814081
3503.112881	373477.026199	48.819085
3503.176725	373452.951275	48.824090
3503.292570	373479.872391	48.829095
3503.433448	373469.496662	48.834100
3503.209074	373462.511116	48.839105
3502.829741	373472.950021	48.844109
3503.315130	373466.666313	48.849114
3503.390747	373459.404398	48.854119
3503.421613	373439.303091	48.859124
3503.152573	373443.288615	48.864129
3502.935927	373432.155359	48.869133
3503.403362	373424.093784	48.874138
3503.174354	373434.839637	48.879143
3503.498353	373428.632312	48.884148
3503.292296	373434.846475	48.889153
3503.005917	373439.903160	48.894157
3503.263353	373435.003724	48.899162
3503.079889	373437.856425	48.904167
3502.941802	373441.261601	48.909172
3503.090261	373439.559211	48.914177
3502.811429	373448.303291	48.919181
3503.136622	373445.326475	48.924186
3503.137009	373436.753644	48.929191
3503.222154	373440.886690	48.934196
3503.477102	373451.098145	48.939201
3502.845328	373422.528785	48.944205
3502.964638	373437.900273	48.949210
3503.226155	373437.528254	48.954215
3502.816442	373435.405324	48.959220
3503.612418	373450.593529	48.964225
3503.641065	373420.622407	48.969229
3503.402099	373408.653199	48.974234
3503.356179	373421.099938	48.979239
3503.436191	373415.999599	48.984244
3503.487823	373419.247594	48.989249
3503.489906	373410.623613	48.994253
3503.082054	373373.547779	48.999258
3502.950029	373397.379184	49.004263
3503.178766	373363.509729	49.009268
3503.372766	373373.451012	49.014273
3503.238370	373376.931926	49.019277
3503.239590	373370.877370	49.024282
3502.998013	373380.505926	49.029287
3503.309521	373376.844427	49.034292
3503.315227	373371.552319	49.039297
3503.032211	373389.785667	49.044301
3503.207458	373378.997465	49.049306
3503.284279	373378.730957	49.054311
3503.483749	373381.014359	49.059316
3503.395017	373387.133666	49.064321
3503.361171	373367.424132	49.069325
3503.572680	373348.947735	49.074330
3503.126367	373341.793742	49.079335
3503.392456	373355.285039	49.084340
3503.434272	373342.533709	49.089345
3503.017422	373343.032080	49.094349
3503.408785	373340.604446	49.099354
3503.414093	373345.996613	49.104359
3503.217066	373339.159355	49.109364
3503.504282	373320.009573	49.114369
3503.407471	373314.428401	49.119373
3503.535269	373299.297674	49.124378
3503.476105	373295.898270	49.129383
3503.481436	373297.474644	49.134388
3503.562639	373296.240774	49.139393
3503.165081	373283.889582	49.144397
3503.357090	373265.975881	49.149402
3503.424030	373271.231122	49.154407
3503.408047	373262.889791	49.159412
3503.096218	373262.404892	49.164417
3503.063688	373264.012691	49.169421
3503.331087	373264.809919	49.174426
3503.204439	373271.672958	49.179431
3502.946314	373275.504141	49.184436
3503.179254	373266.767322	49.189441
3503.006163	373262.724519	49.194445
3503.155285	373269.467650	49.199450
3503.166082	373261.503665	49.204455
3503.332986	373268.396618	49.209460
3503.262698	373264.210372	49.214465
3503.274696	373239.304044	49.219469
3503.631704	373221.516873	49.224474
3503.167094	373235.785120	49.229479
3503.065876	373229.950245	49.234484
3503.309450	373225.892453	49.239489
3503.254308	373225.850313	49.244493
3502.938568	373225.620419	49.249498
3503.084733	373231.804373	49.254503
3502.942955	373237.652262	49.259508
3503.166847	373220.572978	49.264513
3502.721333	373240.561907	49.269517
3503.087338	373225.520692	49.274522
3503.302461	373230.549005	49.279527
3502.904798	373235.368919	49.284532
3503.147509	373236.398999	49.289537
3503.139235	373248.509135	49.294541
3503.237374	373238.623439	49.299546
3503.250495	373242.259116	49.304551
3503.257508	373238.136964	49.309556
3503.166435	373243.391748	49.314561
3503.030658	373247.076400	49.319565
3503.554748	373239.489169	49.324570
3503.023782	373229.550284	49.329575
3503.008182	373223.778191	49.334580
3503.199126	373219.448891	49.339585
3502.874567	373214.310725	49.344589
3502.949509	373208.702388	49.349594
3502.857245	373226.473196	49.354599
3502.987431	373253.086928	49.359604
3503.307886	373241.538016	49.364609
3503.380208	373239.898530	49.369613
3503.092803	373222.569366	49.374618
3503.326928	373224.007822	49.379623
3503.188567	373217.746359	49.384628
3503.094235	373214.708650	49.389633
3503.113109	373215.926744	49.394637
3503.223375	373211.610197	49.399642
3503.240630	373227.252282	49.404647
3503.203381	373214.589727	49.409652
3503.081933	373219.874754	49.414657
3502.990510	373219.990981	49.419661
3503.179027	373220.597170	49.424666
3503.010371	373223.065965	49.429671
3502.915555	373225.802913	49.434676
3503.180820	373229.831191	49.439681
3503.185432	373218.637464	49.444685
3503.253699	373224.401275	49.449690
3503.242050	373222.724184	49.454695
3503.528563	373226.062260	49.459700
3503.504214	373195.743212	49.464705
3502.871318	373190.297641	49.469709
3503.170105	373177.556518	49.474714
3503.098519	373181.638048	49.479719
3503.049158	373193.627502	49.484724
3503.310997	373181.426433	49.489729
3502.691267	373177.454224	49.494733
3503.133558	373175.985201	49.499738
3503.024131	373195.819271	49.504743
3503.267608	373183.086892	49.509748
3503.303560	373188.041778	49.514753
3503.075662	373191.435732	49.519757
3503.153830	373185.979515	49.524762
3503.324887	373190.989360	49.529767
3503.240631	373194.106221	49.534772
3503.382754	373186.884624	49.539777
3503.009056	373192.565670	49.544781
3503.434178	373186.240570	49.549786
3503.167938	373194.804642	49.554791
3503.354872	373193.401424	49.559796
3503.649975	373168.602935	49.564801
3503.084990	373164.215051	49.569805
3503.020128	373154.329663	49.574810
3503.374744	373154.655209	49.579815
3503.466978	373155.607322	49.584820
3503.210767	373156.538199	49.589825
3503.019129	373157.916766	49.594829
3503.152430	373162.169420	49.599834
3503.106201	373159.963581	49.604839
3503.093567	373164.188426	49.609844
3503.437812	373165.736670	49.614849
3503.036769	373173.787842	49.619853
3503.510854	373158.169867	49.624858
3503.243067	373142.618280	49.629863
3503.392191	373135.497322	49.634868
3503.218791	373124.993115	49.639873
3502.656702	373128.821483	49.644877
3503.185779	373126.906282	49.649882
3503.143917	373131.313822	49.654887
3503.243934	373140.634049	49.659892
3503.212486	373126.113523	49.664897
3502.963723	373138.439777	49.669901
3503.222034	373137.254223	49.674906
3503.025856	373141.101065	49.679911
3503.211989	373134.610225	49.684916
3502.922206	373136.004306	49.689921
3503.221086	373140.765003	49.694925
3503.473580	373133.271562	49.699930
3503.541059	373132.039857	49.704935
3503.084990	373145.340112	49.709940
3503.613642	373131.468774	49.714945
3503.230333	373128.400421	49.719949
3503.381827	373120.210659	49.724954
3503.261773	373115.192786	49.729959
3503.257872	373108.706543	49.734964
3503.177028	373114.214113	49.739969
3502.907473	373126.543658	49.744973
3503.269226	373118.575046	49.749978
3503.077341	373122.217701	49.754983
3503.364556	373119.450376	49.759988
3503.368684	373116.549727	49.764993
3503.019364	373123.727815	49.769997
3503.116399	373123.076529	49.775002
3503.255995	373123.461504	49.780007
3503.143331	373109.767850	49.785012
3503.520464	373103.068742	49.790017
3503.241990	373077.877530	49.795021
3503.513998	373072.950310	49.800026
3503.034305	373086.763093	49.805031
3503.074149	373070.068983	49.810036
3503.246736	373077.800548	49.815041
3503.176388	373078.116955	49.820045
3503.224030	373075.438374	49.825050
3503.134089	373083.389509	49.830055
3503.095842	373084.209617	49.835060
3503.467758	373076.595533	49.840065
3503.137620	373099.440873	49.845069
3503.339778	373073.079817	49.850074
3503.415702	373056.532631	49.855079
3502.937661	373082.962789	49.860084
3503.227169	373042.698336	49.865089
3502.962815	373047.777025	49.870093
3503.192647	373041.228386	49.875098
3502.996754	373052.834021	49.880103
3503.210946	373044.150996	49.885108
3503.314970	373040.471388	49.890113
3502.962462	373049.328953	49.895117
3503.153041	373039.250526	49.900122
3503.446193	373047.649887	49.905127
3503.055552	373049.390618	49.910132
3503.273782	373041.520996	49.915137
3503.149932	373047.925731	49.920141
3503.150100	373039.683557	49.925146
3503.134484	373052.837901	49.930151
3503.256777	373051.088753	49.935156
3503.288735	373050.753019	49.940161
3502.944192	373060.143537	49.945165
3503.215024	373046.287486	49.950170
3503.203102	373056.363151	49.955175
3503.213997	373043.209597	49.960180
3503.297879	373022.794443	49.965185
3503.103824	373019.645289	49.970189
3503.255562	373014.864267	49.975194
3503.137155	373018.062857	49.980199
3502.936225	373018.399905	49.985204
3503.334475	373013.096579	49.990209
3503.133505	373030.503072	49.995213
3503.171677	373020.753998	50.000218
3503.188674	373015.994276	50.005223
3503.172412	373023.196049	50.010228
3503.459238	373013.458546	50.015233
3503.216282	373028.327795	50.020237
3503.495863	373022.636208	50.025242
3503.260803	373024.912001	50.030247
3503.296971	373008.116692	50.035252
3503.297417	372990.004204	50.040257
3502.823111	372988.094972	50.045261
3503.251293	372989.731710	50.050266
3503.072040	372995.025903	50.055271
3502.976874	372995.142723	50.060276
3503.247384	372995.634198	50.065281
3503.145669	372994.963450	50.070285
3503.163887	372994.655326	50.075290
3502.934546	372992.045962	50.080295
3502.964149	372993.389562	50.085300
3503.149731	372987.102297	50.090305
3503.185980	373000.426530	50.095309
3503.094451	372998.812935	50.100314
3503.464735	372996.821074	50.105319
3503.361688	372996.277730	50.110324
3503.671725	372993.583105	50.115329
3503.206483	372991.799635	50.120333
3503.476487	372985.499025	50.125338
3503.268083	372967.546736	50.130343
3503.050795	372958.016100	50.135348
3503.448932	372952.254885	50.140353
3503.152875	372956.855259	50.145357
3503.192382	372957.052546	50.150362
3502.871029	372952.727883	50.155367
3503.121594	372953.197073	50.160372
3503.159572	372953.191091	50.165377
3503.232844	372951.373372	50.170381
3503.025983	372963.845687	50.175386
3503.320849	372955.785862	50.180391
3503.044044	372959.569149	50.185396
3503.182193	372946.395449	50.190401
3503.121901	372956.046324	50.195405
3503.280029	372951.035336	50.200410
3503.337616	372951.560470	50.205415
3503.213259	372961.882880	50.210420
3503.320005	372948.408879	50.215425
3503.079003	372937.635484	50.220429
3503.477571	372918.620551	50.225434
3503.090057	372923.184507	50.230439
3503.049256	372922.834834	50.235444
3503.319489	372925.005319	50.240449
3503.210663	372936.368274	50.245453
3503.123399	372928.292532	50.250458
3503.294084	372926.306781	50.255463
3503.431462	372925.013143	50.260468
3503.519367	372921.183439	50.265473
3503.408491	372922.422052	50.270477
3503.551321	372900.267678	50.275482
3503.416569	372894.209107	50.280487
3503.139686	372894.329213	50.285492
3503.579662	372890.698242	50.290497
3503.352087	372892.972859	50.295501
3503.400439	372888.589749	50.300506
3503.884973	372886.121923	50.305511
3503.360784	372869.694964	50.310516
3503.699683	372861.704477	50.315521
3503.175483	372857.895209	50.320525
3503.459505	372852.406408	50.325530
3503.351478	372858.147259	50.330535
3503.247672	372851.193429	50.335540
3503.621657	372820.912900	50.340545
3503.285186	372807.992254	50.345549
3503.458089	372815.876451	50.350554
3503.404800	372809.245335	50.355559
3503.169968	372804.245568	50.360564
3503.336002	372811.825585	50.365569
3503.079686	372821.736427	50.370573
3503.295126	372813.053157	50.375578
3503.157040	372818.976838	50.380583
3502.853232	372820.831047	50.385588
3503.372829	372813.117255	50.390593
3503.212128	372801.644281	50.395597
3503.106448	372793.749497	50.400602
3503.125254	372792.550915	50.405607
3502.863611	372781.551792	50.410612
3502.998067	372784.684989	50.415617
3502.958318	372780.850012	50.420621
3503.287805	372799.088551	50.425626
3503.359266	372788.672749	50.430631
3503.005907	372790.000574	50.435636
3503.537878	372788.110340	50.440641
3503.384142	372788.134663	50.445645
3503.642480	372782.497279	50.450650
3503.474157	372776.901899	50.455655
3503.423292	372779.199467	50.460660
3503.392363	372763.890125	50.465665
3503.045115	372753.438745	50.470669
3503.102401	372738.039133	50.475674
3503.425320	372742.287296	50.480679
3503.204628	372756.186441	50.485684
3503.239781	372742.189473	50.490689
3503.202545	372749.038463	50.495693
3503.230500	372758.548239	50.500698
3503.221136	372758.447985	50.505703
3503.546746	372747.279707	50.510708
3503.447968	372750.348018	50.515713
3502.893541	372733.747713	50.520717
3503.382964	372733.950198	50.525722
3503.195801	372729.807812	50.530727
3503.108135	372714.151276	50.535732
3502.989581	372679.140532	50.540737
3502.776315	372662.257319	50.545741
3502.821049	372626.813696	50.550746
3502.717931	372586.687187	50.555751
3502.546133	372529.654496	50.560756
3502.676312	372492.645468	50.565761
3502.229437	372388.695419	50.570765
3502.268786	372325.498230	50.575770
3501.719823	372214.313707	50.580775
3501.045400	372136.347075	50.585780
3501.435098	372036.257892	50.590785
3500.947689	371921.908384	50.595789
3500.660317	371806.254968	50.600794
3500.189989	371695.641761	50.605799
3499.864167	371568.316994	50.610804
3499.815590	371427.286869	50.615809
3499.062300	371311.960155	50.620813
3498.552826	371179.397209	50.625818
3498.428695	371023.062858	50.630823
3497.966072	370876.219719	50.635828
3497.368644	370714.387675	50.640833
3496.802385	370569.595082	50.645837
3496.426349	370411.899105	50.650842
3495.569271	370262.343218	50.655847
3495.425011	370096.824668	50.660852
3495.047496	369918.698348	50.665857
3494.156207	369764.922995	50.670861
3494.120336	369593.941064	50.675866
3493.482494	369424.707280	50.680871
3492.959113	369238.918057	50.685876
3492.653413	369055.943042	50.690881
3491.995850	368866.204621	50.695885
3491.324006	368673.541873	50.700890
3490.732928	368495.214514	50.705895
3489.980876	368325.816435	50.710900
3490.002820	368108.821135	50.715905
3488.773755	367927.641089	50.720909
3488.350179	367731.780184	50.725914
3487.981268	367545.068906	50.730919
3486.968771	367360.214088	50.735924
3486.780232	367144.010597	50.740929
3485.951187	366935.082062	50.745933
3485.497874	366741.460424	50.750938
3485.036321	366541.427713	50.755943
3484.312560	366329.223051	50.760948
3483.821717	366140.820512	50.765953
3483.042282	365907.784974	50.770957
3482.413245	365728.460255	50.775962
3482.036455	365503.958740	50.780967
3481.373614	365295.861388	50.785972
3480.468568	365085.613237	50.790977
3479.738520	364881.722781	50.795981
3479.522478	364661.237221	50.800986
3478.641607	364449.659250	50.805991
3477.559930	364239.358799	50.810996
3477.318538	364020.757019	50.816001
3476.564596	363812.158445	50.821005
3476.083563	363597.612719	50.826010
3475.394163	363383.200718	50.831015
3474.533597	363172.402459	50.836020
3474.169729	362954.196678	50.841025
3473.513329	362746.493904	50.846029
3472.638459	362528.417808	50.851034
3472.048465	362314.595860	50.856039
3471.370669	362097.758857	50.861044
3470.670974	361886.395034	50.866049
3470.004612	361674.923215	50.871053
3469.174527	361458.947051	50.876058
3468.633640	361246.333887	50.881063
3467.896628	361027.923727	50.886068
3467.569749	360811.661511	50.891073
3466.321427	360603.966572	50.896077
3466.201011	360382.885958	50.901082
3465.727598	360169.468518	50.906087
3464.774543	359950.909487	50.911092
3464.035361	359725.750503	50.916097
3463.301195	359515.043263	50.921101
3462.720166	359285.200534	50.926106
3462.062404	359072.112766	50.931111
3461.143553	358854.052329	50.936116
3460.623327	358642.951246	50.941121
3459.888398	358423.358450	50.946125
3459.279921	358216.239221	50.951130
3458.552489	358003.564986	50.956135
3457.314873	357792.395545	50.961140
3456.995584	357582.326948	50.966145
3456.206267	357376.530618	50.971149
3455.634342	357165.075140	50.976154
3454.881979	356962.503115	50.981159
3454.439930	356750.770876	50.986164
3453.949008	356529.960546	50.991169
3452.879489	356316.086257	50.996173
3452.748453	356092.875894	51.001178
3452.179570	355882.508821	51.006183
3451.384163	355670.878820	51.011188
3450.938474	355447.053708	51.016193
3449.854199	355239.208518	51.021197
3449.511085	355004.193304	51.026202
3448.933587	354792.423424	51.031207
3447.932998	354582.500990	51.036212
3446.934629	354362.932159	51.041217
3446.233056	354156.549038	51.046221
3445.893556	353930.562820	51.051226
3445.025407	353721.532135	51.056231
3444.265156	353512.763499	51.061236
3443.964826	353293.563341	51.066241
3443.233332	353082.167137	51.071245
3442.439318	352864.748371	51.076250
3441.568127	352652.812637	51.081255
3441.077910	352437.329174	51.086260
3440.589602	352225.254848	51.091265
3439.647131	352018.697822	51.096269
3438.833565	351800.717885	51.101274
3438.120162	351592.188773	51.106279
3437.669991	351387.842014	51.111284
3436.969953	351181.116179	51.116289
3436.245927	350969.812222	51.121293
3435.627788	350747.317802	51.126298
3434.961750	350540.100578	51.131303
3433.976098	350327.257529	51.136308
3433.759069	350113.503143	51.141313
3432.857690	349912.149044	51.146317
3432.267024	349701.582622	51.151322
3431.611804	349481.786750	51.156327
3430.812841	349275.145694	51.161332
3430.547755	349054.879220	51.166337
3429.640886	348851.180576	51.171341
3429.160014	348628.554075	51.176346
3428.349357	348428.325567	51.181351
3427.447785	348206.552910	51.186356
3426.950674	347990.289431	51.191361
3426.177460	347791.910736	51.196365
3425.727241	347584.571993	51.201370
3424.744518	347381.898105	51.206375
3423.910762	347175.789316	51.211380
3423.230119	346955.554877	51.216385
3422.537874	346759.832294	51.221389
3421.957493	346550.143277	51.226394
3421.579087	346339.174374	51.231399
3420.391307	346145.029762	51.236404
3420.281510	345922.486711	51.241409
3419.453695	345728.207430	51.246413
3418.868654	345517.420925	51.251418
3418.252303	345310.634769	51.256423
3417.695163	345092.842678	51.261428
3417.044909	344869.439293	51.266433
3416.342071	344664.013567	51.271437
3415.648855	344459.756472	51.276442
3415.097666	344244.302041	51.281447
3413.834326	344038.199157	51.286452
3413.935070	343813.985800	51.291457
3413.144728	343614.628310	51.296461
3412.252368	343407.420982	51.301466
3411.601019	343184.469622	51.306471
3410.533560	342981.310272	51.311476
3410.310383	342765.009586	51.316481
3409.427017	342568.132420	51.321485
3408.828534	342353.875057	51.326490
3408.618196	342147.090133	51.331495
3407.584513	341931.831013	51.336500
3407.315902	341703.799149	51.341505
3406.069075	341504.914202	51.346509
3405.340378	341307.932177	51.351514
3404.764761	341084.248459	51.356519
3404.016627	340877.697054	51.361524
3403.452722	340667.755751	51.366529
3402.526061	340464.794940	51.371533
3402.095699	340252.718346	51.376538
3401.092648	340053.459317	51.381543
3400.608971	339857.961323	51.386548
3400.077845	339643.709448	51.391553
3399.548361	339449.006564	51.396557
3398.613274	339236.828197	51.401562
3398.177165	339017.748060	51.406567
3397.119399	338807.649597	51.411572
3396.771894	338603.522134	51.416577
3395.848533	338407.605579	51.421581
3395.279134	338206.057562	51.426586
3394.447081	338000.859296	51.431591
3393.900509	337792.433203	51.436596
3393.263671	337584.809871	51.441601
3392.875845	337383.256069	51.446605
3391.943433	337179.700325	51.451610
3391.078336	336974.249519	51.456615
3390.424685	336763.800581	51.461620
3390.051155	336554.452243	51.466625
3389.288549	336363.060966	51.471629
3388.668984	336147.564238	51.476634
3388.179305	335948.033309	51.481639
3387.373182	335745.802460	51.486644
3386.907333	335535.981873	51.491649
3385.882877	335327.190888	51.496653
3385.268459	335129.102887	51.501658
3384.683859	334912.909370	51.506663
3383.853824	334714.217832	51.511668
3383.711099	334506.430517	51.516673
3382.692061	334306.469358	51.521677
3382.146634	334080.669511	51.526682
3381.308087	333889.868857	51.531687
3380.361063	333696.640881	51.536692
3380.066299	333480.677118	51.541697
3379.280627	333274.617119	51.546701
3378.430639	333083.561509	51.551706
3378.159198	332874.440436	51.556711
3377.327894	332670.193429	51.561716
3376.698148	332455.756099	51.566721
3375.699232	332260.648507	51.571725
3375.131627	332046.480172	51.576730
3374.745313	331856.595437	51.581735
3373.728933	331657.135569	51.586740
3373.061495	331439.417026	51.591745
3372.465676	331234.034004	51.596749
3371.769117	331039.053534	51.601754
3371.011053	330849.785062	51.606759
3370.573949	330654.431583	51.611764
3369.835154	330444.791869	51.616769
3369.022160	330250.031405	51.621773
3368.429713	330041.462156	51.626778
3368.070441	329850.295024	51.631783
3367.065242	329644.055811	51.636788
3366.611788	329444.551896	51.641793
3365.919073	329247.580314	51.646797
3365.397511	329041.772174	51.651802
3364.580341	328830.103606	51.656807
3363.716558	328631.171641	51.661812
3363.283436	328419.135695	51.666817
3362.537069	328227.338296	51.671821
3362.057966	328030.227976	51.676826
3361.303858	327819.335923	51.681831
3360.424886	327626.463239	51.686836
3359.786241	327423.775428	51.691841
3359.102704	327232.474854	51.696845
3358.481824	327030.572487	51.701850
3357.580799	326821.432286	51.706855
3356.779446	326624.904075	51.711860
3356.284611	326424.609699	51.716865
3355.248205	326233.718974	51.721869
3354.981950	326042.655088	51.726874
3354.712599	325848.103148	51.731879
3353.557994	325648.165787	51.736884
3353.360622	325442.729826	51.741889
3352.838014	325253.079502	51.746893
3352.088235	325045.794889	51.751898
3351.294402	324836.047022	51.756903
3350.253828	324644.618570	51.761908
3349.697032	324443.234322	51.766913
3348.946047	324249.136688	51.771917
3348.459169	324043.768505	51.776922
3347.675222	323857.466271	51.781927
3346.929740	323653.793009	51.786932
3346.503187	323452.054801	51.791937
3345.652173	323262.935670	51.796941
3345.123168	323059.124910	51.801946
3344.533272	322867.035555	51.806951
3343.888021	322657.513407	51.811956
3343.453282	322450.580002	51.816961
3342.613904	322255.193284	51.821965
3341.886475	322063.862292	51.826970
3341.460833	321852.597552	51.831975
3340.258246	321660.755208	51.836980
3339.826615	321451.654710	51.841985
3339.442445	321256.219255	51.846989
3338.553556	321054.726860	51.851994
3337.976877	320862.172729	51.856999
3337.287689	320660.138630	51.862004
3336.948053	320453.873013	51.867009
3335.792175	320260.543489	51.872013
3335.073278	320067.679157	51.877018
3334.667229	319851.314179	51.882023
3334.189284	319660.829806	51.887028
3333.278489	319453.582852	51.892033
3332.431547	319252.156240	51.897037
3331.847004	319056.467687	51.902042
3330.994155	318862.119749	51.907047
3330.441978	318668.996991	51.912052
3329.881015	318465.282761	51.917057
3329.307230	318270.303835	51.922061
3328.088759	318063.713594	51.927066
3327.566449	317866.255818	51.932071
3326.961676	317680.498140	51.937076
3326.211351	317480.605740	51.942081
3325.732805	317300.531069	51.947085
3325.361920	317105.186691	51.952090
3324.467297	316908.778916	51.957095
3323.243795	316697.934243	51.962100
3322.982346	316503.513506	51.967105
3322.380559	316323.965812	51.972109
3321.522236	316123.553021	51.977114
3321.061888	315926.005174	51.982119
3320.179478	315735.678899	51.987124
3319.821668	315538.801594	51.992129
3318.813733	315349.945867	51.997133
3318.423160	315161.195864	52.002138
3317.852992	314947.621480	52.007143
3316.648098	314773.488326	52.012148
3315.989136	314573.677567	52.017153
3315.347366	314395.635175	52.022157
3314.929623	314204.035802	52.027162
3314.469542	314010.532994	52.032167
3313.439260	313809.684571	52.037172
3313.007023	313614.266851	52.042177
3312.255570	313435.730922	52.047181
3311.842747	313228.519632	52.052186
3311.071365	313038.043592	52.057191
3310.083360	312851.191913	52.062196
3309.959468	312649.714171	52.067201
3309.120836	312461.132109	52.072205
3308.234435	312271.335000	52.077210
3307.486121	312071.737458	52.082215
3306.958946	311884.327445	52.087220
3306.664011	311680.328573	52.092225
3305.542054	311498.970644	52.097229
3305.121325	311293.717754	52.102234
3304.453369	311102.610911	52.107239
3303.301497	310918.175593	52.112244
3302.691215	310720.845656	52.117249
3302.350197	310535.110116	52.122253
3301.564596	310351.812807	52.127258
3301.114438	310150.917001	52.132263
3300.495681	309953.867226	52.137268
3299.864390	309752.541027	52.142273
3299.278008	309566.206154	52.147277
3298.299982	309376.342393	52.152282
3297.929940	309183.657432	52.157287
3297.191032	308996.963833	52.162292
3296.398283	308789.957428	52.167297
3295.801879	308592.418066	52.172301
3294.904456	308407.531193	52.177306
3294.147242	308217.783506	52.182311
3293.684101	308025.289718	52.187316
3292.915821	307829.049589	52.192321
3292.102822	307647.738833	52.197325
3291.381942	307448.256540	52.202330
3290.661939	307264.434940	52.207335
3289.966756	307082.009743	52.212340
3289.404926	306889.377062	52.217345
3288.862901	306712.656826	52.222349
3288.316863	306523.153350	52.227354
3287.563014	306315.169088	52.232359
3286.801989	306147.624832	52.237364
3286.611682	305951.876164	52.242369
3285.859440	305764.747053	52.247373
3285.032543	305571.237628	52.252378
3284.465239	305379.393066	52.257383
3283.538655	305183.479624	52.262388
3283.158947	304990.433429	52.267393
3282.574088	304804.447956	52.272397
3281.622496	304610.600387	52.277402
3281.182739	304421.128112	52.282407
3280.805762	304228.360560	52.287412
3280.174854	304021.601215	52.292417
3279.224094	303838.473596	52.297421
3278.577810	303641.189455	52.302426
3278.033329	303432.429256	52.307431
3277.069098	303245.839650	52.312436
3276.563088	303054.899036	52.317441
3275.956957	302855.290082	52.322445
3275.333518	302663.043306	52.327450
3274.610851	302467.068456	52.332455
3273.957934	302286.794952	52.337460
3273.411832	302074.238658	52.342465
3272.275259	301893.506402	52.347469
3271.477030	301705.768129	52.352474
3271.236569	301506.201443	52.357479
3270.380078	301313.047594	52.362484
3269.760177	301133.098597	52.367489
3269.213471	300944.759377	52.372493
3268.351465	300735.460011	52.377498
3267.567170	300553.066127	52.382503
3266.547580	300361.821454	52.387508
3266.189280	300174.801269	52.392513
3265.184487	299990.709917	52.397517
3264.764092	299818.546145	52.402522
3264.350516	299624.734516	52.407527
3263.673875	299437.738397	52.412532
3262.656308	299249.140668	52.417537
3262.066545	299068.242403	52.422541
3261.138485	298879.248114	52.427546
3260.536826	298694.378537	52.432551
3259.644606	298517.755023	52.437556
3259.496535	298337.346410	52.442561
3258.946287	298170.804240	52.447565
3258.257299	297979.300902	52.452570
3258.006347	297774.307041	52.457575
3257.134499	297592.000293	52.462580
3256.194768	297408.176089	52.467585
3255.418220	297222.976145	52.472589
3254.983894	297029.852596	52.477594
3254.220882	296841.135698	52.482599
3253.512986	296661.348818	52.487604
3252.741010	296471.767099	52.492609
3252.198443	296298.040353	52.497613
3251.753646	296108.228261	52.502618
3250.928292	295934.775131	52.507623
3250.125609	295742.701797	52.512628
3249.485291	295564.940604	52.517633
3248.547390	295380.324724	52.522637
3248.256651	295188.500964	52.527642
3247.742752	295016.016478	52.532647
3246.726575	294835.589122	52.537652
3246.425620	294627.187293	52.542657
3245.649108	294458.385714	52.547661
3245.043911	294274.607598	52.552666
3244.392560	294079.656471	52.557671
3243.564989	293893.926760	52.562676
3243.087259	293700.628682	52.567681
3242.311667	293529.839795	52.572685
3241.766234	293336.017300	52.577690
3241.033168	293156.766228	52.582695
3239.840940	292968.419367	52.587700
3239.385562	292782.145999	52.592705
3238.738430	292597.201660	52.597709
3238.096105	292415.669066	52.602714
3237.672656	292239.500829	52.607719
3236.826326	292052.091768	52.612724
3236.316656	291866.997794	52.617729
3235.575718	291694.699529	52.622733
3234.895159	291500.081975	52.627738
3234.430126	291325.957083	52.632743
3233.436939	291137.908421	52.637748
3232.938588	290945.120767	52.642753
3232.489221	290770.534612	52.647757
3231.682154	290587.193107	52.652762
3231.034521	290392.391256	52.657767
3230.206925	290223.824027	52.662772
3229.531458	290039.773713	52.667777
3228.986309	289860.083118	52.672781
3228.391127	289671.333798	52.677786
3227.585965	289492.066122	52.682791
3226.824394	289308.996738	52.687796
3226.183053	289123.565183	52.692801
3225.564145	288935.583182	52.697805
3224.879810	288741.753809	52.702810
3224.375591	288573.007142	52.707815
3223.559085	288390.226046	52.712820
3222.986367	288196.404149	52.717825
3222.395586	288017.381851	52.722829
3221.774548	287830.774801	52.727834
3221.055923	287655.618188	52.732839
3220.072536	287473.015791	52.737844
3219.846319	287275.980520	52.742849
3218.785612	287103.679219	52.747853
3218.135255	286936.381050	52.752858
3217.645135	286746.951227	52.757863
3217.029343	286555.580149	52.762868
3216.195240	286371.883919	52.767873
3215.758175	286203.914976	52.772877
3214.724700	286018.696565	52.777882
3214.460629	285823.092720	52.782887
3213.302924	285657.657012	52.787892
3212.614917	285465.736526	52.792897
3212.258260	285284.078113	52.797901
3211.500243	285111.498826	52.802906
3210.688045	284933.019438	52.807911
3210.159865	284752.279319	52.812916
3209.513145	284573.264245	52.817921
3208.987996	284399.883798	52.822925
3208.072983	284221.955225	52.827930
3207.628040	284032.033117	52.832935
3206.690805	283863.276468	52.837940
3205.972485	283683.406468	52.842945
3205.598427	283513.694689	52.847949
3204.821288	283327.415883	52.852954
3204.515808	283141.800973	52.857959
3203.330297	282975.273579	52.862964
3202.657304	282791.499467	52.867969
3201.901012	282617.034380	52.872973
3201.341991	282432.809164	52.877978
3201.239082	282260.838368	52.882983
3200.193077	282083.490110	52.887988
3199.402841	281898.257113	52.892993
3199.019411	281727.069130	52.897997
3198.062226	281539.621236	52.903002
3197.733006	281377.440360	52.908007
3196.880329	281193.821551	52.913012
3196.287539	281006.748829	52.918017
3195.126302	280840.650003	52.923021
3194.596839	280658.202409	52.928026
3194.397908	280480.898020	52.933031
3193.398288	280321.981053	52.938036
3193.027583	280126.519383	52.943041
3192.458296	279949.120667	52.948045
3191.480638	279781.464493	52.953050
3190.816818	279595.217686	52.958055
3189.999767	279425.574981	52.963060
3189.315936	279240.120795	52.968065
3188.678156	279070.373269	52.973069
3187.763600	278898.912189	52.978074
3187.431851	278729.931187	52.983079
3186.400771	278554.668242	52.988084
3185.814893	278381.092158	52.993089
3185.273349	278208.222154	52.998093
3184.453304	278032.492798	53.003098
3183.922774	277870.597885	53.008103
3183.146073	277709.022056	53.013108
3182.632804	277524.126436	53.018113
3182.214857	277347.518413	53.023117
3181.733418	277177.873290	53.028122
3181.037967	277005.078467	53.033127
3180.259412	276831.889287	53.038132
3179.522642	276639.388448	53.043137
3178.889814	276477.305882	53.048141
3178.298579	276304.367195	53.053146
3177.454272	276117.715610	53.058151
3176.724028	275948.033393	53.063156
3176.485550	275771.014879	53.068161
3175.728618	275595.275403	53.073165
3174.794267	275422.543799	53.078170
3174.340677	275252.232038	53.083175
3173.487652	275079.462103	53.088180
3172.506969	274902.178995	53.093185
3171.987123	274726.070935	53.098189
3171.345823	274558.666817	53.103194
3170.813338	274380.981730	53.108199
3169.930516	274213.182878	53.113204
3169.498856	274037.952292	53.118209
3168.889463	273868.098199	53.123213
3168.093186	273697.382292	53.128218
3167.645865	273507.560841	53.133223
3166.890201	273349.470854	53.138228
3166.476826	273173.575269	53.143233
3165.601670	272990.443340	53.148237
3164.854292	272829.244950	53.153242
3164.152895	272632.943895	53.158247
3163.253687	272474.341873	53.163252
3162.760063	272311.982788	53.168257
3162.196656	272142.885651	53.173261
3161.339825	271956.541951	53.178266
3160.893898	271777.850181	53.183271
3160.155558	271614.944141	53.188276
3159.431797	271433.724084	53.193281
3158.905913	271264.977706	53.198285
3158.414696	271089.578639	53.203290
3157.817448	270913.355928	53.208295
3156.646167	270742.317739	53.213300
3156.277435	270574.870980	53.218305
3155.733257	270409.362138	53.223309
3154.667696	270233.366478	53.228314
3154.332003	270054.199183	53.233319
3153.739670	269878.103264	53.238324
3152.923828	269705.149884	53.243329
3152.079757	269532.251949	53.248333
3151.387222	269366.002771	53.253338
3150.797510	269184.074383	53.258343
3149.871036	269031.131271	53.263348
3149.420731	268856.006414	53.268353
3148.946572	268673.677869	53.273357
3147.884200	268508.022270	53.278362
3147.595426	268340.104988	53.283367
3146.776569	268177.441676	53.288372
3146.132367	268005.862370	53.293377
3145.215052	267832.187004	53.298381
3144.484362	267663.499402	53.303386
3143.972494	267499.386974	53.308391
3143.157104	267343.446974	53.313396
3142.536285	267163.485219	53.318401
3142.193574	267008.209113	53.323405
3141.642927	266843.186187	53.328410
3140.692636	266664.244542	53.333415
3140.080899	266507.610422	53.338420
3139.427669	266340.973949	53.343425
3138.908456	266167.923836	53.348429
3138.142644	265991.576489	53.353434
3137.540839	265827.453419	53.358439
3136.705316	265661.253543	53.363444
3136.306269	265484.568229	53.368449
3135.491347	265321.090317	53.373453
3134.509474	265151.755768	53.378458
3134.243374	264984.727501	53.383463
3133.318331	264823.533877	53.388468
3133.034168	264645.557363	53.393473
3132.306415	264478.194878	53.398477
3131.001510	264308.351524	53.403482
3131.014250	264142.883997	53.408487
3129.826127	263993.371234	53.413492
3129.057597	263814.325712	53.418497
3128.812776	263654.654927	53.423501
3128.009120	263489.265953	53.428506
3127.721028	263326.062127	53.433511
3127.017207	263162.694951	53.438516
3126.379367	262986.048641	53.443521
3125.409169	262823.640628	53.448525
3124.815452	262649.254164	53.453530
3124.448283	262479.619905	53.458535
3123.653863	262315.987352	53.463540
3123.069850	262133.195253	53.468545
3122.483614	261971.363627	53.473549
3121.158602	261801.371952	53.478554
3120.814833	261622.056707	53.483559
3120.365219	261459.898129	53.488564
3119.611331	261293.942157	53.493569
3118.811449	261119.792948	53.498573
3118.162295	260941.519692	53.503578
3117.546165	260791.102999	53.508583
3116.603785	260623.088899	53.513588
3116.094846	260452.230340	53.518593
3115.526412	260293.631249	53.523597
3114.751054	260121.312466	53.528602
3114.084184	259951.701665	53.533607
3113.205510	259793.355708	53.538612
3112.762417	259623.251295	53.543617
3112.086522	259459.168715	53.548621
3111.100390	259304.125384	53.553626
3110.742009	259141.979238	53.558631
3110.029514	258973.700622	53.563636
3109.132905	258806.775567	53.568641
3109.016722	258656.408344	53.573645
3107.573648	258483.381381	53.578650
3107.547582	258332.770894	53.583655
3106.562490	258182.490530	53.588660
3106.230462	258016.240712	53.593665
3105.396096	257846.123054	53.598669
3104.602480	257681.474564	53.603674
3104.634990	257509.946612	53.608679
3103.593688	257361.967743	53.613684
3102.737039	257187.957601	53.618689
3102.439225	257020.760806	53.623693
3101.535234	256855.060763	53.628698
3100.934480	256684.626882	53.633703
3100.169178	256533.650694	53.638708
3099.286308	256362.981571	53.643713
3098.657325	256203.936397	53.648717
3097.964460	256044.341174	53.653722
3097.605801	255875.779673	53.658727
3096.902731	255719.726252	53.663732
3096.210949	255549.715170	53.668737
3095.315901	255390.636323	53.673741
3094.697874	255230.724284	53.678746
3094.081269	255068.036236	53.683751
3093.256316	254900.746287	53.688756
3092.766782	254741.476452	53.693761
3092.094174	254590.181427	53.698765
3091.236107	254424.730750	53.703770
3090.958421	254255.979534	53.708775
3089.919371	254110.422009	53.713780
3089.634630	253942.945534	53.718785
3088.831471	253780.364491	53.723789
3087.569169	253628.959812	53.728794
3087.161079	253463.133167	53.733799
3086.574200	253310.730523	53.738804
3086.013879	253142.585308	53.743809
3085.563063	252995.662230	53.748813
3084.735550	252828.578260	53.753818
3084.331790	252659.975783	53.758823
3083.498086	252511.076354	53.763828
3083.162005	252348.575478	53.768833
3082.236833	252183.799575	53.773837
3081.494874	252018.994834	53.778842
3081.276797	251847.256820	53.783847
3080.058392	251696.025103	53.788852
3079.421545	251536.501247	53.793857
3078.971294	251370.555903	53.798861
3078.015862	251215.259283	53.803866
3077.471195	251042.300440	53.808871
3076.563165	250888.040751	53.813876
3076.183161	250724.937180	53.818881
3075.692067	250565.009189	53.823885
3074.583901	250410.094028	53.828890
3074.389068	250238.328524	53.833895
3073.473347	250091.990853	53.838900
3072.594698	249929.680053	53.843905
3072.067353	249778.238873	53.848909
3071.285737	249615.225449	53.853914
3070.864014	249436.875481	53.858919
3070.215464	249292.024247	53.863924
3069.387246	249130.572144	53.868929
3068.732205	248971.079167	53.873933
3068.054694	248809.221559	53.878938
3067.655458	248653.330091	53.883943
3066.732029	248499.915555	53.888948
3066.050276	248328.178284	53.893953
3065.492276	248178.653486	53.898957
3064.559677	248029.111724	53.903962
3064.413903	247859.021861	53.908967
3063.314626	247709.634131	53.913972
3062.580964	247544.374341	53.918977
3062.020710	247403.942029	53.923981
3061.308221	247237.380477	53.928986
3061.177162	247075.769341	53.933991
3060.330123	246932.887220	53.938996
3059.418000	246747.360322	53.944001
3058.742435	246607.125301	53.949005
3057.987278	246449.993760	53.954010
3057.339266	246284.976532	53.959015
3056.718648	246135.591096	53.964020
3055.965887	245986.150338	53.969025
3055.491890	245829.968163	53.974029
3054.860497	245678.089296	53.979034
3054.091770	245517.701366	53.984039
3053.464934	245357.673153	53.989044
3052.981094	245211.399343	53.994049
3052.370946	245039.909384	53.999053
3051.368686	244888.090101	54.004058
3050.566332	244725.951323	54.009063
3050.162780	244574.190439	54.014068
3049.286743	244420.747397	54.019073
3048.688206	244264.968737	54.024077
3048.154252	244116.183001	54.029082
3047.771355	243950.719239	54.034087
3046.649497	243809.411830	54.039092
3046.035805	243652.133858	54.044097
3045.231101	243491.728627	54.049101
3044.605275	243337.152273	54.054106
3044.279477	243191.288625	54.059111
3043.413814	243024.705610	54.064116
3042.751119	242886.458766	54.069121
3041.917941	242728.427265	54.074125
3041.464419	242572.704123	54.079130
3040.944757	242418.010243	54.084135
3040.185606	242271.503240	54.089140
3039.267741	242105.591811	54.094145
3038.806719	241957.484642	54.099149
3038.046849	241807.693342	54.104154
3037.750524	241647.337364	54.109159
3036.685704	241502.611274	54.114164
3036.172248	241344.199925	54.119169
3035.633767	241194.832717	54.124173
3034.897996	241043.714395	54.129178
3034.803597	240874.338469	54.134183
3033.436836	240725.765026	54.139188
3032.834639	240576.917978	54.144193
3032.206172	240405.106265	54.149197
3031.698270	240255.888201	54.154202
3031.106213	240088.552948	54.159207
3030.272065	239940.278183	54.164212
3029.760839	239782.301495	54.169217
3029.013961	239606.639128	54.174221
3028.065183	239463.221356	54.179226
3027.863956	239303.821196	54.184231
3026.933403	239152.888970	54.189236
3026.103218	238996.771825	54.194241
3025.474584	238843.474987	54.199245
3024.908235	238689.964790	54.204250
3024.611111	238523.349105	54.209255
3023.629845	238377.111357	54.214260
3022.867209	238223.505557	54.219265
3022.315427	238073.049601	54.224269
3021.446638	237917.729481	54.229274
3020.796577	237749.235576	54.234279
3020.030021	237611.011479	54.239284
3019.609837	237458.269263	54.244289
3018.832804	237307.060648	54.249293
3018.270389	237154.545089	54.254298
3017.768347	236996.545486	54.259303
3016.852580	236855.341264	54.264308
3016.361545	236688.835499	54.269313
3015.640380	236530.209223	54.274317
3014.332579	236384.891649	54.279322
3014.304237	236221.547272	54.284327
3013.543058	236062.062282	54.289332
3012.607249	235918.010588	54.294337
3012.185225	235761.196976	54.299341
3011.239192	235618.216787	54.304346
3010.849107	235470.132517	54.309351
3009.807251	235326.123906	54.314356
3009.356675	235172.422247	54.319361
3008.525822	235030.061239	54.324365
3007.873862	234884.641993	54.329370
3007.194373	234731.359189	54.334375
3006.893262	234580.282951	54.339380
3006.321190	234442.490649	54.344385
3005.770681	234290.232097	54.349389
3004.896867	234127.024921	54.354394
3004.397545	233976.923109	54.359399
3003.324895	233830.706256	54.364404
3002.729929	233692.485758	54.369409
3002.281633	233526.589551	54.374413
3001.128088	233375.573702	54.379418
3001.032866	233240.788618	54.384423
3000.190306	233084.249499	54.389428
2999.771667	232935.562442	54.394433
2998.867773	232786.621410	54.399437
2998.170116	232632.708213	54.404442
2997.507130	232478.356915	54.409447
2996.942308	232332.163811	54.414452
2996.221045	232189.560450	54.419457
2995.782226	232030.056435	54.424461
2994.836900	231892.479638	54.429466
2994.543465	231730.457803	54.434471
2993.587382	231578.445994	54.439476
2992.640958	231434.402610	54.444481
2992.137708	231297.240504	54.449485
2991.573694	231143.588691	54.454490
2991.006330	230999.409601	54.459495
2990.370156	230845.285927	54.464500
2989.507230	230699.015275	54.469505
2989.038332	230553.751895	54.474509
2988.322365	230415.122522	54.479514
2988.059665	230246.096386	54.484519
2987.311670	230101.412614	54.489524
2986.400617	229950.287562	54.494529
2986.025807	229788.613061	54.499533
2984.916630	229641.517405	54.504538
2984.738600	229481.009020	54.509543
2983.775769	229332.439391	54.514548
2983.015498	229171.259881	54.519553
2982.697371	229015.332159	54.524557
2982.059343	228872.873610	54.529562
2980.935031	228721.784418	54.534567
2980.324774	228578.048878	54.539572
2979.308989	228418.158817	54.544577
2978.847372	228278.244926	54.549581
2978.307546	228131.341763	54.554586
2977.605396	227973.134256	54.559591
2976.859068	227836.066898	54.564596
2976.134023	227689.346580	54.569601
2975.617513	227527.214943	54.574605
2974.601270	227391.922388	54.579610
2973.939125	227241.526481	54.584615
2973.653036	227113.018754	54.589620
2973.072094	226962.572300	54.594625
2972.592040	226804.204512	54.599629
2971.489319	226666.966319	54.604634
2971.066588	226498.927612	54.609639
2970.381224	226369.313030	54.614644
2969.623948	226228.825542	54.619649
2969.046933	226076.852419	54.624653
2968.143775	225927.782803	54.629658
2967.581375	225785.673929	54.634663
2966.854065	225646.239310	54.639668
2966.265625	225502.187313	54.644673
2965.457955	225346.496623	54.649677
2964.743913	225205.800362	54.654682
2964.533848	225056.253448	54.659687
2963.836098	224922.251196	54.664692
2962.954858	224770.774226	54.669697
2962.855781	224617.442426	54.674701
2961.766508	224471.256505	54.679706
2961.091518	224317.850954	54.684711
2960.706494	224174.303797	54.689716
2959.793055	224014.558811	54.694721
2959.293612	223876.249628	54.699725
2958.277863	223739.791889	54.704730
2957.888632	223576.285836	54.709735
2957.078187	223440.572648	54.714740
2956.362627	223280.925127	54.719745
2956.149123	223133.482818	54.724749
2955.424824	222987.712883	54.729754
2954.595310	222837.631726	54.734759
2953.689451	222694.704384	54.739764
2953.083585	222535.130143	54.744769
2952.589629	222387.924598	54.749773
2951.560589	222248.480088	54.754778
2950.879420	222092.610320	54.759783
2950.361101	221947.204374	54.764788
2949.688092	221813.483588	54.769793
2948.996849	221674.775895	54.774797
2948.273775	221524.082173	54.779802
2947.647993	221373.398810	54.784807
2946.854762	221235.548225	54.789812
2946.412628	221093.925279	54.794817
2945.601355	220951.431781	54.799821
2944.970959	220803.372580	54.804826
2944.525743	220662.667465	54.809831
2943.789222	220515.453055	54.814836
2943.009781	220366.158103	54.819841
2942.486251	220228.075748	54.824845
2941.779555	220087.756815	54.829850
2941.298832	219929.988599	54.834855
2940.433482	219787.938703	54.839860
2939.610432	219637.633789	54.844865
2939.306701	219496.488438	54.849869
2938.491741	219358.402942	54.854874
2937.727727	219206.485685	54.859879
2937.056325	219065.424838	54.864884
2936.355736	218922.803196	54.869889
2935.663965	218769.335191	54.874893
2934.710333	218636.288323	54.879898
2934.517843	218485.936897	54.884903
2933.467242	218351.798477	54.889908
2933.190867	218214.393661	54.894913
2932.702138	218059.405737	54.899917
2931.861805	217916.553648	54.904922
2931.371569	217770.756942	54.909927
2929.984716	217629.303040	54.914932
2929.634858	217502.896334	54.919937
2929.198088	217347.608982	54.924941
2928.323096	217207.131397	54.929946
2927.942412	217069.108883	54.934951
2927.388579	216927.499065	54.939956
2926.273643	216782.427029	54.944961
2925.970738	216646.989715	54.949965
2925.026876	216503.647752	54.954970
2924.463496	216358.336541	54.959975
2923.883104	216215.599528	54.964980
2923.361687	216066.298207	54.969985
2922.643610	215925.212867	54.974989
2922.113757	215791.213319	54.979994
2921.218841	215627.066872	54.984999
2920.437557	215490.829302	54.990004
2919.728255	215355.917108	54.995009
2919.499809	215206.787674	55.000013
2918.405911	215070.715000	55.005018
2917.790103	214922.105746	55.010023
2917.223024	214793.116353	55.015028
2916.736121	214638.606782	55.020033
2916.046053	214499.047392	55.025037
2915.212663	214359.027308	55.030042
2914.908497	214205.482620	55.035047
2913.673424	214067.639645	55.040052
2913.169820	213918.391176	55.045057
2912.574086	213774.528948	55.050061
2911.795387	213653.275855	55.055066
2911.296729	213495.919684	55.060071
2910.518609	213364.395386	55.065076
2910.011200	213219.680329	55.070081
2909.065017	213064.368908	55.075085
2908.380268	212933.123442	55.080090
2907.925177	212776.882175	55.085095
2907.146233	212645.384914	55.090100
2906.369295	212513.365755	55.095105
2905.776946	212366.311367	55.100109
2905.154591	212225.218739	55.105114
2904.784331	212084.697449	55.110119
2903.943658	211953.325924	55.115124
2903.179107	211809.469317	55.120129
2902.740189	211670.143496	55.125133
2901.662610	211530.269977	55.130138
2901.148353	211385.331019	55.135143
2900.649621	211246.346517	55.140148
2899.932514	211102.751279	55.145153
2899.411523	210959.876250	55.150157
2898.663867	210822.446686	55.155162
2897.946489	210682.416192	55.160167
2897.036853	210547.125662	55.165172
2896.222300	210408.867574	55.170177
2895.556215	210258.864215	55.175181
2895.031179	210132.181149	55.180186
2894.713853	209988.639712	55.185191
2893.890807	209861.393462	55.190196
2892.980167	209720.772079	55.195201
2892.676920	209579.736664	55.200205
2891.364309	209449.985108	55.205210
2890.971125	209311.039109	55.210215
2890.560098	209175.303534	55.215220
2889.656777	209045.577122	55.220225
2889.043019	208899.743328	55.225229
2888.019710	208774.389214	55.230234
2888.015635	208629.655895	55.235239
2886.874396	208496.773791	55.240244
2886.220243	208364.514850	55.245249
2886.057735	208225.331162	55.250253
2885.316824	208097.248311	55.255258
2884.329813	207955.192194	55.260263
2883.791135	207826.059734	55.265268
2882.813628	207685.924532	55.270273
2882.522604	207549.613602	55.275277
2881.840117	207423.330167	55.280282
2881.159299	207283.238020	55.285287
2880.391499	207150.172494	55.290292
2879.726282	207015.296534	55.295297
2879.508394	206872.892127	55.300301
2878.605564	206741.923369	55.305306
2877.866422	206602.452948	55.310311
2876.964631	206473.062742	55.315316
2876.501967	206335.394556	55.320321
2875.872197	206187.597251	55.325325
2875.422585	206064.016080	55.330330
2875.008078	205919.850644	55.335335
2873.810004	205782.987433	55.340340
2873.291602	205652.049322	55.345345
2872.646109	205507.412415	55.350349
2871.889353	205372.745616	55.355354
2871.153529	205240.226591	55.360359
2870.522405	205098.286443	55.365364
2869.732780	204969.556312	55.370369
2869.666895	204825.083864	55.375373
2868.592738	204700.535464	55.380378
2868.287815	204556.508781	55.385383
2867.405815	204422.945768	55.390388
2866.457764	204279.759738	55.395393
2865.882546	204142.801795	55.400397
2865.077389	204016.965119	55.405402
2864.613535	203883.057184	55.410407
2863.794828	203748.925776	55.415412
2862.930520	203616.189053	55.420417
2862.550484	203483.185071	55.425421
2861.767389	203350.283400	55.430426
2861.571475	203207.248230	55.435431
2860.692086	203077.327615	55.440436
2859.875762	202955.300144	55.445441
2859.422129	202816.595427	55.450445
2858.503167	202679.580925	55.455450
2857.836990	202547.604359	55.460455
2857.269622	202419.506570	55.465460
2856.598801	202283.293657	55.470465
2856.468972	202134.804111	55.475469
2855.555095	202006.418545	55.480474
2854.851606	201865.808717	55.485479
2854.070510	201737.479105	55.490484
2853.260825	201586.655346	55.495489
2852.683622	201450.925959	55.500493
2851.777158	201326.396668	55.505498
2851.088278	201191.894537	55.510503
2850.275235	201065.620369	55.515508
2849.693876	200932.450758	55.520513
2849.467078	200798.639956	55.525517
2848.503496	200678.575103	55.530522
2848.058221	200543.577880	55.535527
2847.472080	200416.416685	55.540532
2846.459575	200279.613854	55.545537
2846.026745	200140.187240	55.550541
2845.272888	200010.164909	55.555546
2844.951077	199867.387394	55.560551
2844.302927	199738.303375	55.565556
2843.358474	199608.121318	55.570561
2842.661238	199468.178404	55.575565
2841.966982	199344.409028	55.580570
2841.450789	199197.184829	55.585575
2840.677300	199063.732126	55.590580
2840.229597	198936.221661	55.595585
2839.856993	198802.108057	55.600589
2838.584062	198663.861767	55.605594
2838.166211	198538.141753	55.610599
2837.308843	198407.083548	55.615604
2836.414340	198274.008293	55.620609
2836.080654	198132.344372	55.625613
2835.098637	198008.407360	55.630618
2834.499154	197877.118766	55.635623
2833.833056	197752.127077	55.640628
2833.306637	197633.615901	55.645633
2832.701853	197490.316979	55.650637
2832.187131	197361.612093	55.655642
2831.650090	197225.988864	55.660647
2830.806593	197096.547770	55.665652
2829.869744	196970.048430	55.670657
2829.702312	196823.450051	55.675661
2828.630292	196703.093266	55.680666
2828.018966	196572.878696	55.685671
2827.595596	196439.288165	55.690676
2826.624126	196303.863391	55.695681
2826.013647	196174.260466	55.700685
2825.144196	196055.374595	55.705690
2824.567002	195922.356914	55.710695
2823.836852	195794.224472	55.715700
2823.286059	195667.590858	55.720705
2822.897922	195535.167735	55.725709
2822.092136	195410.725531	55.730714
2821.407396	195270.842802	55.735719
2820.757304	195139.887295	55.740724
2819.753930	195013.403326	55.745729
2819.520879	194886.670447	55.750733
2818.691792	194758.085498	55.755738
2818.134030	194628.261858	55.760743
2817.556963	194503.251261	55.765748
2816.765948	194372.778124	55.770753
2816.047745	194236.644394	55.775757
2815.092094	194114.366734	55.780762
2814.698573	193987.012618	55.785767
2814.065624	193865.231589	55.790772
2813.326180	193728.720893	55.795777
2813.049496	193593.549622	55.800781
2811.959331	193475.213737	55.805786
2811.645542	193337.987800	55.810791
2810.743464	193204.150821	55.815796
2810.092289	193073.671668	55.820801
2809.424380	192935.968535	55.825805
2808.686681	192820.670223	55.830810
2808.163554	192687.321747	55.835815
2807.567224	192558.362091	55.840820
2807.065133	192433.879217	55.845825
2806.278948	192304.339571	55.850829
2805.255331	192183.018985	55.855834
2804.736972	192047.483079	55.860839
2804.394760	191913.879039	55.865844
2803.379279	191787.774195	55.870849
2803.155098	191660.819140	55.875853
2802.408613	191531.949593	55.880858
2801.670855	191399.262062	55.885863
2800.941814	191269.665231	55.890868
2800.485362	191136.857533	55.895873
2799.859478	190995.717994	55.900877
2798.649235	190870.893243	55.905882
2798.252846	190745.469180	55.910887
2797.757380	190604.119292	55.915892
2796.848521	190485.100367	55.920897
2796.172927	190352.265928	55.925901
2795.544276	190232.897907	55.930906
2794.951562	190091.666717	55.935911
2794.021490	189970.985748	55.940916
2793.434798	189836.306588	55.945921
2793.050534	189706.952008	55.950925
2792.523258	189587.518661	55.955930
2791.707776	189448.004056	55.960935
2791.072053	189316.832860	55.965940
2790.120202	189191.602638	55.970945
2789.770352	189067.765946	55.975949
2789.120617	188940.923675	55.980954
2788.809442	188794.206543	55.985959
2787.775126	188666.764351	55.990964
2787.173120	188539.673879	55.995969
2786.402394	188394.430240	56.000973
2785.460690	188282.075854	56.005978
2784.901286	188143.084353	56.010983
2783.896571	188019.710368	56.015988
2783.360937	187897.967197	56.020993
2783.035788	187772.450691	56.025997
2782.190748	187643.988992	56.031002
2781.857637	187509.238188	56.036007
2780.777693	187391.500959	56.041012
2779.952762	187262.668196	56.046017
2779.670820	187128.711886	56.051021
2779.048769	187012.009922	56.056026
2778.325617	186879.968898	56.061031
2777.694803	186747.735522	56.066036
2776.637607	186620.646077	56.071041
2776.724594	186501.581350	56.076045
2775.666573	186372.622616	56.081050
2775.078695	186243.017310	56.086055
2774.466231	186114.332230	56.091060
2773.458221	185990.442623	56.096065
2773.262817	185847.558461	56.101069
2772.245789	185726.698753	56.106074
2771.762985	185602.676138	56.111079
2771.194213	185475.474374	56.116084
2770.548108	185350.180718	56.121089
2769.729235	185221.047448	56.126093
2769.155585	185090.603568	56.131098
2768.717919	184957.721464	56.136103
2767.929214	184827.376014	56.141108
2767.167445	184703.209237	56.146113
2767.014561	184566.708497	56.151117
2765.721728	184438.466706	56.156122
2765.443230	184311.883767	56.161127
2764.755477	184181.460604	56.166132
2763.905689	184054.752616	56.171137
2763.083132	183921.247610	56.176141
2762.407709	183789.704188	56.181146
2762.261613	183659.845542	56.186151
2761.204866	183529.775319	56.191156
2760.137921	183398.256907	56.196161
2759.729720	183270.272733	56.201165
2758.961087	183142.803967	56.206170
2758.642834	183020.734198	56.211175
2757.804444	182893.735152	56.216180
2757.053505	182767.663960	56.221185
2756.787266	182636.949621	56.226189
2755.784815	182507.993244	56.231194
2755.348875	182376.963101	56.236199
2754.824295	182245.565771	56.241204
2753.984098	182123.224992	56.246209
2753.218385	181992.642572	56.251213
2752.397827	181860.606373	56.256218
2751.525022	181729.443842	56.261223
2751.033927	181601.833850	56.266228
2750.485329	181489.319722	56.271233
2750.080180	181353.008826	56.276237
2749.114891	181237.355823	56.281242
2748.505145	181097.872618	56.286247
2747.739951	180971.567209	56.291252
2747.368639	180849.143047	56.296257
2746.880620	180707.504833	56.301261
2745.927699	180586.305634	56.306266
2745.521344	180445.583920	56.311271
2744.729694	180324.945041	56.316276
2743.822745	180190.485397	56.321281
2743.401676	180065.807194	56.326285
2742.626624	179949.478818	56.331290
2742.125058	179813.366164	56.336295
2741.339558	179688.454230	56.341300
2740.359694	179550.522918	56.346305
2739.992314	179429.068911	56.351309
2739.043346	179303.840569	56.356314
2738.531229	179182.486513	56.361319
2737.878723	179057.771611	56.366324
2737.309921	178922.104940	56.371329
2736.985976	178788.091628	56.376333
2736.035711	178672.379619	56.381338
2735.513983	178538.678259	56.386343
2734.655515	178408.528516	56.391348
2733.808555	178282.244062	56.396353
2733.529836	178149.866431	56.401357
2733.046658	178027.290068	56.406362
2732.166559	177897.374291	56.411367
2731.450012	177772.050112	56.416372
2730.358612	177639.154143	56.421377
2729.986187	177510.990731	56.426381
2729.238607	177388.241903	56.431386
2728.901680	177258.280248	56.436391
2728.280443	177137.623525	56.441396
2727.358600	177001.497535	56.446401
2726.918305	176872.227575	56.451405
2726.107266	176745.458785	56.456410
2725.541705	176622.505336	56.461415
2724.692797	176484.868669	56.466420
2724.156624	176361.860470	56.471425
2723.956519	176222.506621	56.476429
2722.804892	176097.052942	56.481434
2722.070444	175968.252139	56.486439
2721.570969	175842.263507	56.491444
2720.832011	175712.166921	56.496449
2720.263190	175593.566854	56.501453
2719.736416	175456.976423	56.506458
2718.934070	175330.261517	56.511463
2718.115562	175196.732461	56.516468
2717.445144	175076.789118	56.521473
2717.047582	174946.704499	56.526477
2716.023718	174820.636760	56.531482
2715.244215	174691.910733	56.536487
2715.113355	174563.514793	56.541492
2713.995054	174430.900599	56.546497
2713.756270	174303.222088	56.551501
2713.003433	174173.565066	56.556506
2712.457927	174049.128205	56.561511
2712.045698	173908.734869	56.566516
2711.095734	173783.472634	56.571521
2710.402116	173642.387159	56.576525
2709.446069	173518.220468	56.581530
2709.165842	173378.838238	56.586535
2708.712470	173254.465565	56.591540
2707.630313	173131.044977	56.596545
2706.783907	172991.690199	56.601549
2706.396229	172868.605541	56.606554
2705.361136	172727.755451	56.611559
2704.979888	172606.832597	56.616564
2704.076719	172478.374935	56.621569
2703.956270	172346.131043	56.626573
2703.062127	172220.915771	56.631578
2702.372278	172097.359963	56.636583
2701.840124	171960.909503	56.641588
2701.120189	171832.234163	56.646593
2700.692741	171697.434012	56.651597
2699.937583	171566.412412	56.656602
2699.236324	171435.128368	56.661607
2698.513294	171312.419631	56.666612
2697.488201	171185.320828	56.671617
2697.279939	171049.025716	56.676621
2696.433049	170921.161951	56.681626
2695.697301	170788.321344	56.686631
2695.466389	170655.045145	56.691636
2694.750080	170533.456900	56.696641
2693.850852	170401.025027	56.701645
2693.031968	170262.069829	56.706650
2692.736974	170131.984805	56.711655
2692.103475	169991.386174	56.716660
2691.322356	169867.228782	56.721665
2690.897612	169725.885912	56.726669
2690.257981	169608.993621	56.731674
2689.262850	169464.779081	56.736679
2688.952616	169331.507302	56.741684
2687.771758	169193.249137	56.746689
2687.347158	169053.587306	56.751693
2686.643636	168925.847336	56.756698
2685.879627	168803.992358	56.761703
2685.418905	168674.625216	56.766708
2684.433940	168541.361350	56.771713
2683.999954	168405.925199	56.776717
2683.228585	168279.596938	56.781722
2682.331989	168142.683630	56.786727
2682.106088	168009.377685	56.791732
2681.316104	167883.727649	56.796737
2680.780974	167756.320990	56.801741
2680.225163	167621.441020	56.806746
2679.328668	167483.156757	56.811751
2678.931341	167358.565275	56.816756
2678.156317	167218.418934	56.821761
2677.881919	167077.227406	56.826765
2676.941913	166944.801302	56.831770
2676.153111	166803.641431	56.836775
2675.788923	166672.676392	56.841780
2674.875075	166532.567326	56.846785
2674.196587	166392.052750	56.851789
2673.469717	166262.875926	56.856794
2672.663787	166125.167252	56.861799
2672.499311	166000.238236	56.866804
2671.720902	165867.790360	56.871809
2671.061401	165721.070187	56.876813
2670.346734	165589.083679	56.881818
2669.714922	165458.012731	56.886823
2669.272826	165317.426630	56.891828
2668.563735	165188.276167	56.896833
2667.778878	165040.599487	56.901837
2667.086963	164902.966309	56.906842
2666.591798	164762.683179	56.911847
2665.718820	164620.222601	56.916852
2664.840675	164484.349735	56.921857
2664.400871	164350.963625	56.926861
2663.717547	164217.870877	56.931866
2663.311880	164084.721913	56.936871
2662.696018	163935.802292	56.941876
2661.856548	163800.828591	56.946881
2661.423639	163655.136099	56.951885
2660.530118	163521.329031	56.956890
2659.413304	163375.962154	56.961895
2659.132100	163236.401156	56.966900
2658.239864	163112.563570	56.971905
2658.022514	162964.512957	56.976909
2657.430334	162825.447814	56.981914
2656.486475	162695.974658	56.986919
2655.759578	162560.123176	56.991924
2655.059973	162425.488447	56.996929
2654.685609	162279.385370	57.001933
2653.426063	162150.078622	57.006938
2653.034967	162003.674179	57.011943
2652.760134	161863.875920	57.016948
2651.363159	161736.283406	57.021953
2651.142959	161589.446736	57.026957
2650.136504	161459.759115	57.031962
2649.589974	161329.198130	57.036967
2648.939660	161192.538735	57.041972
2648.285479	161050.477141	57.046977
2648.064123	160909.784189	57.051981
2646.983955	160793.561758	57.056986
2646.372178	160649.854990	57.061991
2645.999664	160509.759686	57.066996
2645.211382	160373.138022	57.072001
2644.610458	160233.029148	57.077005
2643.625753	160094.252972	57.082010
2643.051649	159968.596029	57.087015
2642.705603	159835.351703	57.092020
2641.821062	159700.044658	57.097025
2641.505053	159551.337346	57.102029
2640.589656	159424.617659	57.107034
2639.823392	159295.370323	57.112039
2639.210851	159140.990838	57.117044
2638.183668	159014.074229	57.122049
2637.781634	158872.439147	57.127053
2637.355825	158738.042045	57.132058
2636.698157	158598.864026	57.137063
2636.266360	158467.914098	57.142068
2635.492910	158320.810038	57.147073
2634.952834	158181.831177	57.152077
2634.079428	158047.889041	57.157082
2633.340863	157910.531798	57.162087
2632.814268	157758.026305	57.167092
2632.237989	157624.483675	57.172097
2631.627196	157483.789927	57.177101
2630.942993	157346.693278	57.182106
2630.112575	157197.098691	57.187111
2629.728495	157054.591053	57.192116
2629.052772	156916.554069	57.197121
2628.615389	156764.076985	57.202125
2627.286972	156615.631660	57.207130
2626.690061	156483.355238	57.212135
2626.242452	156341.381829	57.217140
2625.537041	156205.805838	57.222145
2624.895387	156068.122819	57.227149
2623.987955	155926.401960	57.232154
2623.607602	155783.288867	57.237159
2623.043540	155642.569870	57.242164
2622.142481	155507.485287	57.247169
2621.734718	155363.361372	57.252173
2620.641944	155221.545711	57.257178
2619.760444	155087.514770	57.262183
2619.794101	154940.360932	57.267188
2618.782504	154803.224708	57.272193
2618.134109	154657.667406	57.277197
2617.522680	154523.684900	57.282202
2617.153170	154377.944798	57.287207
2616.616654	154236.210403	57.292212
2615.735134	154097.251460	57.297217
2615.359903	153950.802297	57.302221
2614.708110	153804.168794	57.307226
2613.939255	153655.330058	57.312231
2613.443051	153505.101427	57.317236
2612.563211	153301.688388	57.322241
2611.918595	153171.110365	57.327245
2611.205939	153018.490461	57.332250
2610.730794	152877.667291	57.337255
2610.224825	152702.213096	57.342260
2608.921295	152589.574797	57.347265
2608.642643	152433.228173	57.352269
2607.860339	152281.054864	57.357274
2607.073711	152146.702954	57.362279
2606.730621	151987.267310	57.367284
2605.985653	151847.368303	57.372289
2605.621580	151699.084325	57.377293
2604.487559	151547.414998	57.382298
2603.877779	151398.535800	57.387303
2603.233310	151260.301112	57.392308
2602.422816	151117.110985	57.397313
2602.043213	150960.469616	57.402317
2601.219089	150822.303378	57.407322
2600.264672	150690.742078	57.412327
2599.914924	150527.666870	57.417332
2598.868218	150388.304894	57.422337
2598.672755	150243.597667	57.427341
2597.870325	150109.510833	57.432346
2597.341617	149974.860090	57.437351
2596.896717	149810.202158	57.442356
2595.973920	149670.823637	57.447361
2595.543769	149524.491871	57.452365
2595.101108	149384.606390	57.457370
2594.017309	149225.187254	57.462375
2593.613909	149068.990915	57.467380
2592.577768	148928.095754	57.472385
2592.002332	148777.952236	57.477389
2591.411897	148633.022509	57.482394
2590.589224	148489.019865	57.487399
2590.492862	148330.567108	57.492404
2589.398024	148194.196151	57.497409
2589.104998	148045.955779	57.502413
2588.374669	147894.684451	57.507418
2587.254490	147740.438237	57.512423
2586.886970	147584.967860	57.517428
2586.333988	147444.638125	57.522433
2585.600757	147289.659234	57.527437
2584.708210	147147.122507	57.532442
2584.076312	147006.273463	57.537447
2583.431723	146842.119963	57.542452
2582.709161	146709.788486	57.547457
2582.262479	146551.679697	57.552461
2581.609208	146411.332317	57.557466
2580.768285	146268.816796	57.562471
2580.104521	146116.857188	57.567476
2579.457776	145974.147031	57.572481
2579.122064	145821.819171	57.577485
2578.440671	145674.693512	57.582490
2577.537601	145524.414012	57.587495
2577.102743	145366.563477	57.592500
2575.943074	145233.532321	57.597505
2575.527146	145072.655845	57.602509
2574.830318	144925.180352	57.607514
2574.200256	144776.004882	57.612519
2573.702273	144623.746707	57.617524
2572.822274	144487.357789	57.622529
2572.305088	144338.560464	57.627533
2571.350804	144187.139179	57.632538
2571.122114	144042.834052	57.637543
2570.330076	143893.917226	57.642548
2569.587875	143745.183829	57.647553
2569.138733	143610.903416	57.652557
2568.481424	143453.021632	57.657562
2567.435646	143300.170610	57.662567
2567.315269	143148.762062	57.667572
2566.354005	142997.347735	57.672577
2565.748196	142849.651721	57.677581
2564.876246	142690.524497	57.682586
2564.315332	142547.371806	57.687591
2564.064222	142393.281208	57.692596
2563.040220	142246.899615	57.697601
2562.291958	142094.287018	57.702605
2562.019906	141940.036847	57.707610
2561.105511	141803.360360	57.712615
2560.456728	141645.143497	57.717620
2559.603200	141495.066420	57.722625
2559.071508	141337.074027	57.727629
2558.623508	141191.749794	57.732634
2557.652929	141044.552354	57.737639
2557.390827	140881.500771	57.742644
2556.567335	140747.241475	57.747649
2556.226707	140592.475392	57.752653
2555.627549	140441.041847	57.757658
2554.506196	140279.044499	57.762663
2554.269708	140114.722447	57.767668
2553.189084	139975.463242	57.772673
2552.605471	139816.762840	57.777677
2552.083345	139664.342693	57.782682
2551.319282	139508.264419	57.787687
2551.112372	139347.296093	57.792692
2549.690909	139197.930342	57.797697
2549.552496	139043.877117	57.802701
2548.731641	138903.832149	57.807706
2547.923699	138744.855375	57.812711
2547.330082	138585.095900	57.817716
2546.553216	138442.212946	57.822721
2545.953997	138280.321589	57.827725
2545.571669	138135.637037	57.832730
2544.750809	137976.882415	57.837735
2544.365772	137809.420470	57.842740
2543.638975	137659.495034	57.847745
2543.154297	137496.052581	57.852749
2542.347328	137343.168623	57.857754
2541.536686	137197.108257	57.862759
2540.891555	137032.283633	57.867764
2540.442174	136879.790071	57.872769
2540.010426	136716.216530	57.877773
2538.734690	136555.115195	57.882778
2538.019763	136389.136484	57.887783
2537.630621	136242.315371	57.892788
2536.607474	136093.118224	57.897793
2536.076446	135936.170781	57.902797
2535.409726	135784.720981	57.907802
2534.688234	135636.850371	57.912807
2534.007344	135473.742509	57.917812
2533.357814	135335.034005	57.922817
2532.893023	135166.545454	57.927821
2532.476820	135018.235815	57.932826
2531.774582	134861.232401	57.937831
2531.236309	134691.538749	57.942836
2530.390283	134544.811343	57.947841
2529.815612	134378.377310	57.952845
2529.165085	134231.214023	57.957850
2528.636761	134052.719374	57.962855
2528.052024	133900.301046	57.967860
2527.016100	133742.454721	57.972865
2526.654903	133580.869357	57.977869
2526.103428	133422.465319	57.982874
2525.550671	133268.508267	57.987879
2524.965825	133100.025456	57.992884
2524.074931	132933.815069	57.997889
2523.185255	132775.150665	58.002893
2522.726443	132602.674984	58.007898
2521.882194	132437.095224	58.012903
2521.342072	132282.785843	58.017908
2520.840557	132124.381116	58.022913
2520.290302	131949.167551	58.027917
2519.436697	131784.037665	58.032922
2518.518573	131624.139429	58.037927
2518.185732	131467.782053	58.042932
2517.631085	131306.748363	58.047937
2516.450601	131145.497238	58.052941
2515.804118	130981.698306	58.057946
2515.404790	130816.679921	58.062951
2514.510029	130652.693632	58.067956
2513.786623	130503.554415	58.072961
2513.434402	130334.695598	58.077965
2512.483761	130177.249405	58.082970
2511.852802	130007.471451	58.087975
2511.550468	129849.314707	58.092980
2510.891535	129693.171327	58.097985
2510.178302	129520.526259	58.102989
2509.411481	129362.814221	58.107994
2508.748012	129196.056467	58.112999
2508.168461	129026.568472	58.118004
2507.315462	128876.290052	58.123009
2506.854563	128707.712349	58.128013
2506.087020	128549.878050	58.133018
2505.478249	128394.051552	58.138023
2504.735034	128210.624086	58.143028
2503.872614	128056.528836	58.148033
2503.136561	127893.524317	58.153037
2502.527869	127742.603752	58.158042
2502.032617	127584.223833	58.163047
2501.633990	127405.725529	58.168052
2500.936142	127254.872579	58.173057
2500.274469	127087.974905	58.178061
2499.510582	126922.796211	58.183066
2498.920408	126766.353725	58.188071
2498.042014	126593.397604	58.193076
2497.299347	126432.345870	58.198081
2497.103297	126258.877346	58.203085
2496.250973	126103.953345	58.208090
2495.619653	125944.245684	58.213095
2495.027580	125783.212029	58.218100
2493.885489	125617.275764	58.223105
2493.652976	125460.936498	58.228109
2493.193454	125283.490385	58.233114
2492.298882	125121.987956	58.238119
2491.509124	124965.460504	58.243124
2490.851388	124803.312907	58.248129
2490.398868	124621.527083	58.253133
2490.012772	124462.246473	58.258138
2489.087761	124299.395063	58.263143
2488.442922	124132.106593	58.268148
2487.629937	123966.433108	58.273153
2487.005383	123797.175278	58.278157
2486.292411	123638.751361	58.283162
2485.157442	123465.906763	58.288167
2484.690587	123306.506152	58.293172
2484.095441	123153.971009	58.298177
2483.491367	122985.591241	58.303181
2482.700777	122819.794352	58.308186
2481.943908	122671.668339	58.313191
2481.508434	122502.871280	58.318196
2480.870965	122346.360434	58.323201
2480.546148	122178.043109	58.328205
2479.707484	122010.113036	58.333210
2479.104660	121855.504210	58.338215
2478.050489	121684.728078	58.343220
2477.608527	121529.536990	58.348225
2477.262827	121357.876158	58.353229
2476.596027	121192.717408	58.358234
2475.928773	121026.378956	58.363239
2475.398370	120859.575479	58.368244
2473.928411	120693.201312	58.373249
2473.479045	120524.254072	58.378253
2472.958090	120372.529488	58.383258
2472.254470	120210.074446	58.388263
2471.433142	120046.597964	58.393268
2470.793325	119883.734903	58.398273
2470.504322	119716.830627	58.403277
2469.409045	119557.209520	58.408282
2468.535495	119404.765642	58.413287
2468.346538	119241.282860	58.418292
2467.796087	119086.790012	58.423297
2467.146887	118918.176874	58.428301
2466.675110	118760.734405	58.433306
2465.795620	118579.826008	58.438311
2465.418212	118417.527258	58.443316
2464.518680	118263.875439	58.448321
2464.081840	118086.639179	58.453325
2463.249418	117925.691543	58.458330
2462.548918	117762.978398	58.463335
2462.081980	117577.612724	58.468340
2461.325402	117426.761587	58.473345
2460.511625	117252.593228	58.478349
2459.957175	117079.222816	58.483354
2458.984889	116913.384403	58.488359
2458.676235	116755.065108	58.493364
2457.942206	116591.330096	58.498369
2457.684894	116418.342344	58.503373
2456.837569	116253.802307	58.508378
2456.118689	116082.756097	58.513383
2455.614622	115914.323769	58.518388
2454.562811	115739.054638	58.523393
2453.865622	115572.660889	58.528397
2453.360452	115409.665213	58.533402
2452.783397	115248.732072	58.538407
2452.227202	115076.194356	58.543412
2451.228286	114910.189183	58.548417
2450.746247	114728.413635	58.553421
2450.258452	114567.235854	58.558426
2449.245829	114393.905636	58.563431
2448.798866	114228.985276	58.568436
2448.189935	114055.149130	58.573441
2447.532650	113877.723284	58.578445
2447.075769	113719.719381	58.583450
2446.242978	113563.273860	58.588455
2445.755851	113369.247319	58.593460
2444.568475	113210.188316	58.598465
2444.174085	113038.127636	58.603469
2443.805418	112868.336086	58.608474
2442.911934	112707.659790	58.613479
2442.338950	112521.275466	58.618484
2441.545168	112358.891148	58.623489
2440.801947	112179.891730	58.628493
2440.053543	112024.375399	58.633498
2439.129191	111861.151953	58.638503
2438.937583	111684.296182	58.643508
2438.357629	111532.874873	58.648513
2437.868403	111352.711571	58.653517
2437.147570	111167.947378	58.658522
2435.982057	111007.763109	58.663527
2435.497389	110835.706644	58.668532
2435.042507	110676.630298	58.673537
2434.310874	110486.390107	58.678541
2433.529229	110330.071121	58.683546
2432.892995	110156.501416	58.688551
2432.620826	109980.520980	58.693556
2431.503552	109820.419311	58.698561
2431.052238	109648.467418	58.703565
2430.576182	109470.270286	58.708570
2429.960444	109305.035090	58.713575
2428.589657	109117.978090	58.718580
2427.938336	108959.191526	58.723585
2427.536678	108800.118952	58.728589
2427.003055	108631.074434	58.733594
2426.141282	108455.668026	58.738599
2425.919787	108279.787019	58.743604
2425.187103	108118.100045	58.748609
2424.320186	107946.137242	58.753613
2424.254694	107773.801159	58.758618
2423.140119	107595.991847	58.763623
2422.429681	107415.619846	58.768628
2421.661178	107247.015629	58.773633
2421.155250	107074.164283	58.778637
2420.369813	106913.737353	58.783642
2419.353053	106742.714214	58.788647
2419.257506	106569.071790	58.793652
2418.621588	106405.775743	58.798657
2417.786503	106229.391534	58.803661
2417.093941	106058.848496	58.808666
2416.563064	105881.352728	58.813671
2415.941763	105715.299175	58.818676
2415.060175	105537.563367	58.823681
2414.660899	105364.967583	58.828685
2414.141739	105201.597819	58.833690
2413.136024	105027.045029	58.838695
2412.894418	104841.707564	58.843700
2412.119880	104680.475500	58.848705
2411.293829	104497.352370	58.853709
2410.988837	104329.976818	58.858714
2410.006183	104159.880387	58.863719
2409.455669	103978.462236	58.868724
2408.793581	103792.438353	58.873729
2408.171020	103630.237754	58.878733
2407.307622	103445.650548	58.883738
2406.657906	103271.511055	58.888743
2406.215322	103098.995765	58.893748
2405.469268	102927.785927	58.898753
2404.714518	102743.523237	58.903757
2404.237895	102558.881689	58.908762
2403.501529	102391.753244	58.913767
2403.011741	102208.328190	58.918772
2402.083803	102028.520096	58.923777
2401.602039	101862.306613	58.928781
2401.104533	101677.472348	58.933786
2400.059623	101498.771621	58.938791
2399.750989	101316.358845	58.943796
2399.052454	101151.922888	58.948801
2398.134454	100983.342660	58.953805
2397.621224	100799.247351	58.958810
2396.693548	100620.985168	58.963815
2396.238378	100442.624079	58.968820
2395.146780	100271.647133	58.973825
2394.910854	100081.532036	58.978829
2394.266196	99909.839925	58.983834
2393.363569	99733.642096	58.988839
2393.223094	99553.189219	58.993844
2392.432976	99382.672165	58.998849
2391.885239	99212.181378	59.003853
2391.059982	99031.213224	59.008858
2390.177864	98849.589530	59.013863
2389.760375	98666.022533	59.018868
2388.769445	98484.393618	59.023873
2388.257745	98306.172231	59.028877
2387.863258	98135.233874	59.033882
2386.638297	97959.716015	59.038887
2386.371973	97780.096208	59.043892
2385.565793	97612.131867	59.048897
2384.777877	97433.992804	59.053901
2383.932840	97259.967637	59.058906
2383.167675	97074.229762	59.063911
2382.709168	96902.892231	59.068916
2382.026342	96739.804597	59.073921
2381.910326	96562.923067	59.078925
2381.249902	96391.507261	59.083930
2380.339749	96214.386525	59.088935
2379.643641	96022.107774	59.093940
2378.825132	95849.167384	59.098945
2378.326826	95676.336102	59.103949
2377.705058	95501.965647	59.108954
2376.602976	95335.282760	59.113959
2376.449242	95143.122126	59.118964
2375.582862	94987.794087	59.123969
2374.877194	94806.301675	59.128973
2374.730768	94623.682059	59.133978
2373.311806	94450.054964	59.138983
2373.129891	94265.008781	59.143988
2372.423696	94093.706558	59.148993
2371.868395	93916.103821	59.153997
2371.092382	93733.819591	59.159002
2370.206805	93564.553719	59.164007
2369.805650	93386.968814	59.169012
2369.181968	93209.331833	59.174017
2368.398149	93035.158523	59.179021
2367.764435	92854.000347	59.184026
2367.055653	92685.423348	59.189031
2366.431641	92508.312001	59.194036
2365.511008	92324.775079	59.199041
2364.941614	92147.975006	59.204045
2364.503520	91967.693476	59.209050
2363.433521	91795.059054	59.214055
2363.159729	91612.503430	59.219060
2362.139802	91445.824031	59.224065
2361.540222	91267.330193	59.229069
2361.267198	91093.611158	59.234074
2360.378077	90908.603719	59.239079
2359.944036	90742.819543	59.244084
2359.137121	90570.647597	59.249089
2358.489318	90387.819086	59.254093
2357.603094	90203.451185	59.259098
2357.044827	90035.460304	59.264103
2356.381341	89861.426213	59.269108
2356.046247	89691.861939	59.274113
2355.317732	89514.588459	59.279117
2354.355586	89325.408913	59.284122
2353.837468	89151.560336	59.289127
2353.109658	88968.870548	59.294132
2352.385259	88802.874561	59.299137
2351.613478	88623.136349	59.304141
2351.057287	88450.174328	59.309146
2350.309645	88276.958761	59.314151
2349.869017	88091.251199	59.319156
2349.378674	87927.177436	59.324161
2348.717280	87738.185976	59.329165
2348.333096	87566.243453	59.334170
2347.497050	87396.510337	59.339175
2346.817753	87202.194965	59.344180
2345.873377	87025.540348	59.349185
2345.258244	86848.904714	59.354189
2344.638546	86682.312582	59.359194
2343.674731	86496.429171	59.364199
2343.134976	86312.990426	59.369204
2342.458940	86151.862995	59.374209
2341.802022	85972.388651	59.379213
2341.464454	85791.667119	59.384218
2340.514736	85624.425605	59.389223
2339.903956	85436.872694	59.394228
2339.342922	85262.606003	59.399233
2339.046440	85085.826683	59.404237
2338.177562	84911.630701	59.409242
2337.120019	84728.623664	59.414247
2336.560786	84546.033607	59.419252
2336.055525	84368.450343	59.424257
2335.244300	84193.091183	59.429261
2334.811715	84015.905021	59.434266
2333.995076	83842.520882	59.439271
2333.195864	83667.088130	59.444276
2332.450016	83497.587334	59.449281
2332.083794	83311.015942	59.454285
2331.425873	83132.535578	59.459290
2330.427101	82958.591818	59.464295
2330.233626	82781.232362	59.469300
2329.470090	82607.349287	59.474305
2328.779844	82427.929346	59.479309
2328.289341	82255.514332	59.484314
2327.773202	82066.385588	59.489319
2327.094450	81892.666134	59.494324
2326.446951	81706.559250	59.499329
2325.872261	81523.757084	59.504333
2325.071119	81333.862614	59.509338
2323.970068	81153.295617	59.514343
2323.685992	80970.281120	59.519348
2322.928272	80797.020621	59.524353
2322.320240	80616.075924	59.529357
2321.836075	80426.614796	59.534362
2321.042541	80248.960111	59.539367
2320.565841	80063.804135	59.544372
2319.847099	79887.699653	59.549377
2319.038323	79698.828988	59.554381
2318.875359	79515.858840	59.559386
2317.804053	79330.892444	59.564391
2317.374077	79144.254455	59.569396
2316.756754	78964.954296	59.574401
2315.847110	78778.516088	59.579405
2314.975520	78590.609746	59.584410
2314.356369	78404.737203	59.589415
2313.981709	78219.201440	59.594420
2313.208577	78042.557430	59.599425
2312.551729	77857.639986	59.604429
2312.098457	77667.635418	59.609434
2311.015593	77487.173733	59.614439
2310.615020	77299.724153	59.619444
2309.742806	77118.446622	59.624449
2309.287161	76935.178426	59.629453
2308.830793	76748.015233	59.634458
2308.151845	76553.558144	59.639463
2307.469292	76375.805402	59.644468
2306.559032	76188.548269	59.649473
2306.276179	75999.400300	59.654477
2305.392576	75813.587010	59.659482
2304.495915	75630.717334	59.664487
2303.912413	75435.242117	59.669492
2303.041395	75252.859655	59.674497
2302.464211	75075.285376	59.679501
2301.589919	74890.391452	59.684506
2300.972433	74709.608297	59.689511
2300.259600	74520.383990	59.694516
2299.501141	74345.999978	59.699521
2298.916003	74164.906160	59.704525
2298.699426	73992.713694	59.709530
2297.735836	73808.357062	59.714535
2297.222075	73621.485401	59.719540
2296.577839	73439.457234	59.724545
2295.849261	73254.789693	59.729549
2295.027544	73070.201982	59.734554
2294.376316	72891.923930	59.739559
2294.147315	72711.737053	59.744564
2293.530695	72534.704692	59.749569
2292.705499	72345.430113	59.754573
2292.033527	72155.543909	59.759578
2291.281400	71973.527251	59.764583
2290.367269	71794.838301	59.769588
2289.770694	71609.309938	59.774593
2289.188493	71421.354914	59.779597
2288.676501	71233.118161	59.784602
2287.854419	71074.754738	59.789607
2287.531346	70882.988437	59.794612
2286.550550	70698.017308	59.799617
2285.690274	70515.796861	59.804621
2285.657272	70328.240225	59.809626
2284.617475	70153.437243	59.814631
2284.037742	69962.411030	59.819636
2283.560367	69772.314207	59.824641
2282.544547	69588.670212	59.829645
2281.933892	69413.311727	59.834650
2281.218451	69232.606690	59.839655
2280.695921	69037.311436	59.844660
2280.095873	68873.356863	59.849665
2279.434293	68676.586181	59.854669
2278.826422	68487.054571	59.859674
2277.928185	68313.771975	59.864679
2277.383251	68129.984691	59.869684
2276.583633	67947.075541	59.874689
2276.043776	67763.094585	59.879693
2275.479329	67578.935606	59.884698
2274.927929	67399.348889	59.889703
2274.689746	67209.448117	59.894708
2273.556121	67025.337165	59.899713
2272.873086	66836.802549	59.904718
2272.552125	66643.168140	59.909722
2271.677321	66460.044305	59.914727
2271.255197	66268.690545	59.919732
2270.435646	66084.231620	59.924737
2269.794590	65888.904533	59.929742
2268.912319	65700.282806	59.934746
2267.925732	65524.341507	59.939751
2267.735456	65333.017277	59.944756
2267.034578	65144.122112	59.949761
2265.931458	64954.469388	59.954766
2265.796751	64774.419950	59.959770
2264.903118	64593.080463	59.964775
2264.367805	64401.063551	59.969780
2263.728335	64209.008098	59.974785
2262.823639	64026.985536	59.979790
2262.435192	63843.315658	59.984794
2261.544034	63660.762557	59.989799
2261.143241	63465.235315	59.994804
2260.212647	63284.427028	59.999809
2259.251144	63117.393866	60.004814
2259.241010	62920.195667	60.009818
2258.296599	62733.518970	60.014823
2257.983041	62539.978735	60.019828
2257.006767	62352.307290	60.024833
2256.393096	62167.400878	60.029838
2255.898650	61980.916672	60.034842
2254.928762	61801.065836	60.039847
2254.373353	61605.265749	60.044852
2254.005967	61416.566845	60.049857
2253.069830	61235.516288	60.054862
2252.288207	61034.354361	60.059866
2251.517968	60850.891206	60.064871
2251.097520	60665.247159	60.069876
2250.526591	60481.765500	60.074881
2249.582524	60294.058826	60.079886
2249.127835	60110.397766	60.084890
2248.291609	59932.123166	60.089895
2247.854561	59729.853865	60.094900
2247.004715	59542.285402	60.099905
2246.125050	59356.863277	60.104910
2245.953214	59176.987015	60.109914
2244.792435	59000.159172	60.114919
2244.591661	58807.987902	60.119924
2243.987376	58612.717471	60.124929
2243.429526	58428.196773	60.129934
2242.654183	58238.217827	60.134938
2241.814264	58068.735262	60.139943
2241.477338	57858.915448	60.144948
2240.635497	57676.140562	60.149953
2239.624162	57488.181691	60.154958
2239.466865	57295.658395	60.159962
2238.565237	57111.794019	60.164967
2238.155826	56908.266135	60.169972
2237.324481	56725.847129	60.174977
2236.519005	56539.798981	60.179982
2235.796620	56353.869292	60.184986
2234.938558	56171.412553	60.189991
2234.608943	55974.259266	60.194996
2234.036402	55787.124791	60.200001
2233.095797	55591.275097	60.205006
2232.890916	55410.364772	60.210010
2232.098367	55229.732988	60.215015
2231.570564	55036.589587	60.220020
2230.592515	54838.247591	60.225025
2230.005808	54638.927990	60.230030
2229.175380	54451.474684	60.235034
2228.396290	54281.678823	60.240039
2227.812706	54087.003773	60.245044
2227.583844	53900.660021	60.250049
2226.761458	53721.633248	60.255054
2226.168757	53526.440375	60.260058
2225.329305	53334.617512	60.265063
2224.553790	53150.716024	60.270068
2223.867333	52965.365747	60.275073
2223.584025	52769.844014	60.280078
2223.048969	52579.028208	60.285082
2222.275553	52390.726526	60.290087
2221.622244	52198.212249	60.295092
2220.823573	52007.649960	60.300097
2219.717749	51817.189031	60.305102
2219.666967	51620.525991	60.310106
2218.807391	51449.291931	60.315111
2218.182847	51250.028305	60.320116
2217.651118	51061.075757	60.325121
2216.507795	50876.338312	60.330126
2216.456830	50667.486124	60.335130
2215.291174	50488.539586	60.340135
2214.614928	50306.524351	60.345140
2214.389035	50113.243318	60.350145
2213.521717	49936.966247	60.355150
2212.840868	49728.886132	60.360154
2212.597912	49542.757390	60.365159
2211.980255	49346.215574	60.370164
2210.956866	49147.617578	60.375169
2210.102592	48972.822173	60.380174
2209.713233	48762.805878	60.385178
2208.943010	48579.795084	60.390183
2208.325937	48380.530688	60.395188
2207.882801	48200.243034	60.400193
2206.954899	48005.454493	60.405198
2206.093407	47805.472987	60.410202
2205.400094	47618.227503	60.415207
2204.947180	47422.841786	60.420212
2204.000220	47248.236277	60.425217
2203.219538	47064.297051	60.430222
2202.930779	46869.656902	60.435226
2202.114801	46682.459796	60.440231
2201.585470	46486.264707	60.445236
2201.184327	46306.008735	60.450241
2200.468145	46116.046875	60.455246
2199.677770	45920.642809	60.460250
2198.684019	45728.451879	60.465255
2198.626499	45541.421813	60.470260
2197.912846	45358.255246	60.475265
2196.684817	45173.091081	60.480270
2196.564888	44964.636599	60.485274
2195.493513	44780.349973	60.490279
2194.655589	44592.818149	60.495284
2194.107585	44403.151850	60.500289
2193.542108	44224.999123	60.505294
2192.924144	44023.488278	60.510298
2192.048426	43843.364628	60.515303
2191.568670	43651.956304	60.520308
2190.901691	43467.360127	60.525313
2190.272735	43278.787865	60.530318
2189.865189	43087.728509	60.535322
2189.172165	42898.964991	60.540327
2188.520337	42710.143239	60.545332
2187.933518	42519.479107	60.550337
2187.149284	42326.764465	60.555342
2186.445774	42132.091239	60.560346
2185.453367	41943.037824	60.565351
2185.377555	41756.940005	60.570356
2184.740715	41554.800040	60.575361
2183.682373	41382.120915	60.580366
2183.002231	41174.525042	60.585370
2182.153626	40987.739169	60.590375
2181.469276	40807.733865	60.595380
2180.789248	40613.080456	60.600385
2180.253309	40418.969225	60.605390
2179.773929	40238.303433	60.610394
2179.039162	40054.279499	60.615399
2178.397650	39854.291429	60.620404
2177.866365	39677.465594	60.625409
2176.844286	39484.856996	60.630414
2176.743935	39295.435217	60.635418
2175.748755	39113.837189	60.640423
2175.280036	38916.430035	60.645428
2174.307877	38718.676640	60.650433
2173.805672	38538.971492	60.655438
2173.419929	38350.527113	60.660442
2172.425007	38158.610560	60.665447
2171.897401	37964.412194	60.670452
2171.403612	37783.820610	60.675457
2170.385995	37593.275066	60.680462
2169.807296	37397.328847	60.685466
2169.027232	37212.217477	60.690471
2168.137254	37020.957919	60.695476
2167.580739	36831.318352	60.700481
2167.171908	36638.619572	60.705486
2166.688191	36459.012650	60.710490
2165.967231	36277.278322	60.715495
2165.280348	36078.206640	60.720500
2164.557195	35894.821965	60.725505
2163.902047	35703.167148	60.730510
2163.290063	35510.330206	60.735514
2162.519205	35319.448875	60.740519
2161.887529	35131.525233	60.745524
2161.242417	34942.768201	60.750529
2160.536931	34750.737175	60.755534
2159.760868	34553.434673	60.760538
2159.065212	34388.292171	60.765543
2158.443694	34193.738258	60.770548
2158.079666	33996.802106	60.775553
2157.364478	33825.114563	60.780558
2156.780338	33616.956343	60.785562
2155.797881	33423.841997	60.790567
2155.008632	33239.092128	60.795572
2154.663240	33058.202443	60.800577
2154.076365	32863.562225	60.805582
2153.621973	32663.312434	60.810586
2152.417753	32489.578261	60.815591
2151.717925	32301.533096	60.820596
2151.165120	32115.764324	60.825601
2150.623472	31932.419835	60.830606
2150.056684	31737.927169	60.835610
2149.312103	31554.132401	60.840615
2148.920658	31359.524741	60.845620
2148.355510	31176.274565	60.850625
2147.523593	30980.211752	60.855630
2146.973827	30786.759418	60.860634
2145.883772	30589.756274	60.865639
2145.348732	30403.925021	60.870644
2144.543216	30210.905581	60.875649
2143.919682	30024.528617	60.880654
2143.501148	29837.340756	60.885658
2142.800432	29653.226968	60.890663
2141.895249	29472.250658	60.895668
2141.468646	29287.329669	60.900673
2140.420731	29094.502494	60.905678
2140.202256	28894.676762	60.910682
2139.385139	28706.828895	60.915687
2138.901819	28517.483120	60.920692
2138.378823	28334.651503	60.925697
2137.481609	28152.878163	60.930702
2136.622813	27949.056604	60.935706
2135.770119	27762.177917	60.940711
2135.260752	27566.201353	60.945716
2134.421142	27393.170447	60.950721
2133.440470	27211.375107	60.955726
2133.071805	27021.621059	60.960730
2132.372884	26848.606050	60.965735
2131.755655	26655.283839	60.970740
2131.399694	26473.714417	60.975745
2130.290144	26304.619160	60.980750
2129.537934	26116.393806	60.985754
2129.019346	25933.190601	60.990759
2128.292911	25750.800391	60.995764
2127.776823	25580.647170	61.000769
2126.873124	25394.499024	61.005774
2126.808626	25206.986306	61.010778
2125.826550	25039.886958	61.015783
2124.963113	24853.214325	61.020788
2124.643698	24664.300819	61.025793
2123.527810	24496.185156	61.030798
2123.033158	24305.431274	61.035802
2122.059406	24130.757343	61.040807
2121.546628	23952.522550	61.045812
2121.042760	23785.095916	61.050817
2120.176190	23600.735612	61.055822
2119.949710	23427.459107	61.060826
2119.061707	23257.513608	61.065831
2117.935321	23089.187042	61.070836
2117.820840	22900.152167	61.075841
2117.050224	22727.487628	61.080846
2116.549939	22542.203426	61.085850
2115.446415	22361.709757	61.090855
2114.952674	22182.726660	61.095860
2114.212661	22021.056231	61.100865
2113.453256	21848.270007	61.105870
2113.213860	21664.057743	61.110874
2112.645776	21485.563342	61.115879
2111.946190	21310.648784	61.120884
2111.104194	21135.903249	61.125889
2110.278083	20960.778942	61.130894
2109.750665	20781.138072	61.135898
2108.906975	20616.463136	61.140903
2108.456758	20438.882478	61.145908
2107.375295	20256.242587	61.150913
2106.375982	20088.106293	61.155918
2106.055208	19926.279531	61.160922
2105.188622	19754.588055	61.165927
2104.432824	19595.129148	61.170932
2103.673589	19414.090443	61.175937
2102.788999	19260.360440	61.180942
2102.722111	19093.971310	61.185946
2101.712556	18940.171919	61.190951
2101.050911	18766.449652	61.195956
2100.475285	18608.832515	61.200961
2099.424234	18455.624712	61.205966
2099.090561	18288.455242	61.210970
2098.074117	18135.171686	61.215975
2097.229684	17973.627032	61.220980
2096.765773	17816.875223	61.225985
2096.087252	17673.132423	61.230990
2095.333106	17512.511080	61.235994
2094.318725	17374.845032	61.240999
2093.730343	17217.916942	61.246004
2093.014920	17070.300588	61.251009
2092.032356	16948.632315	61.256014
2091.129644	16783.870837	61.261018
2090.383512	16660.378103	61.266023
2089.223357	16541.157926	61.271028
2088.336914	16419.064967	61.276033
2087.318339	16313.389789	61.281038
2086.304156	16195.463711	61.286042
2084.394038	16107.991190	61.291047
2083.380260	16009.422575	61.296052
2082.415107	15939.990081	61.301057
2081.431837	15871.853129	61.306062
2080.640138	15791.326063	61.311066
2079.398281	15738.092574	61.316071
2078.823411	15680.424962	61.321076
2078.024154	15620.096332	61.326081
2077.399916	15557.495196	61.331086
2076.764893	15505.010054	61.336090
2076.370877	15450.565983	61.341095
2076.284732	15401.249412	61.346100
2075.292642	15336.578321	61.351105
2074.427488	15277.697446	61.356110
2074.147395	15217.611613	61.361114
2073.519516	15168.031323	61.366119
2072.589473	15104.695749	61.371124
2071.809326	15049.733585	61.376129
2071.266915	14995.265841	61.381134
2070.979285	14931.660051	61.386138
2070.010579	14900.145658	61.391143
2069.829900	14825.251510	61.396148
2069.092217	14767.024103	61.401153
2068.340630	14719.281302	61.406158
2068.144067	14653.507435	61.411162
2067.337394	14599.532024	61.416167
2066.921520	14537.138755	61.421172
2065.878264	14469.118971	61.426177
2065.629971	14420.060448	61.431182
2064.941251	14351.847212	61.436186
2063.854309	14296.471989	61.441191
2063.357680	14229.375725	61.446196
2063.007610	14168.211674	61.451201
2061.995622	14112.664722	61.456206
2061.421130	14053.922272	61.461210
2060.834199	13999.080113	61.466215
2060.434560	13935.168426	61.471220
2059.723210	13869.517495	61.476225
2059.116345	13814.991182	61.481230
2058.475366	13753.603844	61.486234
2057.810766	13688.769185	61.491239
2057.112408	13630.862542	61.496244
2056.744146	13569.259867	61.501249
2055.950935	13510.569111	61.506254
2055.660685	13444.760757	61.511258
2054.590467	13378.490408	61.516263
2054.407808	13312.864614	61.521268
2053.297227	13240.495705	61.526273
2052.750419	13189.696939	61.531278
2052.300526	13109.785131	61.536282
2051.193830	13055.847874	61.541287
2050.560508	12991.018620	61.546292
2049.955233	12941.000751	61.551297
2049.000511	12890.401474	61.556302
2048.777583	12826.634082	61.561306
2047.907488	12756.823371	61.566311
2047.318130	12706.377622	61.571316
2046.943359	12641.602932	61.576321
2045.938331	12585.665993	61.581326
2045.612942	12515.835646	61.586330
2045.022508	12446.481885	61.591335
2044.159128	12383.352801	61.596340
2043.797150	12323.500851	61.601345
2042.882250	12259.969532	61.606350
2042.338907	12198.383619	61.611354
2041.513590	12146.122215	61.616359
2040.884064	12071.876705	61.621364
2040.360191	12008.832015	61.626369
2039.512581	11961.716655	61.631374
2039.228991	11891.484455	61.636378
2038.084440	11835.907194	61.641383
2037.383746	11768.002260	61.646388
2036.998475	11711.710005	61.651393
2036.339960	11647.791999	61.656398
2035.717474	11592.814933	61.661402
2035.305410	11526.680122	61.666407
2034.693944	11464.978596	61.671412
2033.909728	11389.753159	61.676417
2032.709463	11330.226745	61.681422
2032.233101	11272.471114	61.686426
2031.712701	11207.332520	61.691431
2030.729514	11150.866596	61.696436
2030.232484	11088.317590	61.701441
2029.430286	11028.545747	61.706446
2029.055025	10968.335150	61.711450
2028.486981	10923.093644	61.716455
2027.758280	10855.978982	61.721460
2027.178908	10789.921682	61.726465
2026.201486	10746.570282	61.731470
2025.940667	10675.514997	61.736474
2025.186905	10610.275568	61.741479
2024.145399	10559.423099	61.746484
2023.643846	10497.538844	61.751489
2022.941199	10438.942968	61.756494
2022.648949	10369.438585	61.761498
2021.991612	10312.567468	61.766503
2021.362526	10252.752690	61.771508
2020.882348	10177.804591	61.776513
2019.871630	10125.814927	61.781518
2019.512565	10064.150087	61.786522
2018.817836	9996.705055	61.791527
2018.045019	9943.587899	61.796532
2017.419638	9878.810177	61.801537
2016.841009	9818.550451	61.806542
2015.941473	9760.052769	61.811546
2015.295233	9696.384487	61.816551
2014.629025	9633.708605	61.821556
2013.971017	9572.935437	61.826561
2013.203799	9510.133695	61.831566
2012.697583	9456.005543	61.836570
2012.354988	9383.117668	61.841575
2011.110459	9335.540591	61.846580
2010.776671	9259.902052	61.851585
2010.097439	9205.164405	61.856590
2009.592295	9144.449580	61.861594
2008.675667	9080.170432	61.866599
2007.996020	9011.134586	61.871604
2007.703617	8960.600990	61.876609
2006.720267	8906.527272	61.881614
2006.078930	8834.255528	61.886618
2005.249714	8783.896081	61.891623
2004.470303	8724.082856	61.896628
2004.083109	8661.521388	61.901633
2003.360526	8596.559519	61.906638
2003.066179	8530.307170	61.911642
2002.190775	8471.505390	61.916647
2001.615711	8409.063545	61.921652
2001.363072	8348.114259	61.926657
2000.533270	8285.613563	61.931662
1999.926839	8210.935941	61.936666
1999.210563	8148.282904	61.941671
1998.205168	8090.975703	61.946676
1997.656470	8034.684890	61.951681
1997.032788	7964.376091	61.956686
1996.252873	7903.533601	61.961690
1995.243994	7845.312810	61.966695
1994.948721	7789.212264	61.971700
1994.448206	7721.576663	61.976705
1993.348264	7673.096850	61.981710
1992.800839	7603.080969	61.986714
1992.290696	7541.330982	61.991719
1991.821196	7482.753854	61.996724
1991.160619	7422.940398	62.001729
1990.377760	7367.859124	62.006734
1989.738447	7284.555925	62.011738
1989.254362	7225.677632	62.016743
1988.149544	7167.843107	62.021748
1987.951230	7108.052211	62.026753
1986.795222	7048.729870	62.031758
1986.419632	6988.594477	62.036762
1985.500538	6941.376497	62.041767
1984.875499	6868.858088	62.046772
1984.547961	6815.612373	62.051777
1983.102078	6751.039574	62.056782
1982.931379	6691.131595	62.061786
1981.834460	6635.729779	62.066791
1981.187017	6574.149164	62.071796
1981.198308	6526.739880	62.076801
1980.256452	6466.130910	62.081806
1980.007409	6407.275350	62.086810
1979.207047	6342.710733	62.091815
1978.621174	6288.711236	62.096820
1977.741218	6224.609373	62.101825
1976.848617	6170.338746	62.106830
1976.713752	6107.821313	62.111834
1975.829686	6049.344033	62.116839
1974.965169	5982.421703	62.121844
1974.590462	5924.116480	62.126849
1973.316628	5878.534148	62.131854
1972.749586	5814.720411	62.136858
1972.078412	5768.002396	62.141863
1971.723425	5703.487406	62.146868
1971.295198	5648.476918	62.151873
1970.326255	5581.709431	62.156878
1970.265498	5520.213608	62.161882
1969.292533	5465.154598	62.166887
1968.250534	5410.126469	62.171892
1967.896332	5341.327728	62.176897
1967.188417	5296.159801	62.181902
1966.673648	5232.241691	62.186906
1966.017729	5171.795351	62.191911
1965.178773	5110.439733	62.196916
1964.285682	5052.684782	62.201921
1963.547847	4997.481358	62.206926
1963.183634	4931.422168	62.211930
1962.544272	4872.060485	62.216935
1961.700477	4822.428618	62.221940
1961.245508	4763.172975	62.226945
1960.562989	4701.989827	62.231950
1959.730671	4631.875862	62.236954
1959.045236	4580.725887	62.241959
1958.551668	4528.928882	62.246964
1958.140032	4458.808910	62.251969
1957.268251	4409.298029	62.256974
1956.678869	4348.945457	62.261978
1956.122009	4291.603872	62.266983
1954.969533	4236.694678	62.271988
1954.637094	4176.060699	62.276993
1953.863822	4122.352041	62.281998
1953.302463	4066.867783	62.287002
1952.576451	4005.673142	62.292007
1951.842482	3956.540978	62.297012
1951.302873	3886.164075	62.302017
1950.454919	3833.609512	62.307022
1949.946593	3768.124954	62.312026
1949.216204	3721.060848	62.317031
1948.668030	3654.343370	62.322036
1947.756792	3597.496076	62.327041
1946.928779	3548.992979	62.332046
1946.537875	3501.667493	62.337050
1945.833479	3437.031771	62.342055
1945.039681	3388.986700	62.347060
1944.388703	3333.049421	62.352065
1943.458341	3278.461083	62.357070
1943.146142	3215.836585	62.362074
1942.559157	3166.265774	62.367079
1941.489005	3122.479024	62.372084
1941.035853	3063.695232	62.377089
1940.453957	3017.008859	62.382094
1939.923110	2962.682405	62.387098
1939.158636	2901.379405	62.392103
1938.507329	2847.228643	62.397108
1938.013873	2793.517509	62.402113
1937.269145	2746.499824	62.407118
1936.664351	2687.857537	62.412122
1936.201349	2630.332487	62.417127
1935.623411	2574.571835	62.422132
1934.701256	2517.601148	62.427137
1933.831015	2469.730529	62.432142
1933.461917	2409.343097	62.437146
1932.449652	2357.617175	62.442151
1931.761777	2304.784840	62.447156
1931.057906	2250.680910	62.452161
1930.260493	2194.558321	62.457166
1929.521390	2152.153186	62.462170
1929.262809	2095.468369	62.467175
1928.438895	2049.646763	62.472180
1928.040484	1984.535981	62.477185
1927.091665	1951.244910	62.482190
1926.406854	1882.613429	62.487194
1925.772739	1835.495175	62.492199
1925.214178	1785.293708	62.497204
1924.755039	1727.580779	62.502209
1924.144833	1683.453305	62.507214
1923.286460	1640.732677	62.512218
1922.345141	1591.152498	62.517223
1921.508573	1537.811925	62.522228
1921.031778	1480.736756	62.527233
1920.156775	1432.130673	62.532238
1919.617147	1404.927173	62.537242
1919.281281	1340.299805	62.542247
1918.566465	1294.792864	62.547252
1918.098251	1245.889432	62.552257
1917.054158	1201.501122	62.557262
1916.610349	1136.784555	62.562266
1916.258206	1091.233299	62.567271
1915.129468	1044.447660	62.572276
1914.706885	991.137214	62.577281
1913.698604	956.619138	62.582286
1913.343359	895.245434	62.587290
1912.556560	859.919706	62.592295
1911.533522	807.341565	62.597300
1911.056725	754.060308	62.602305
1910.086808	720.566470	62.607310
1909.513661	679.503373	62.612314
1908.919124	631.032078	62.617319
1908.171432	588.136136	62.622324
1907.796886	547.319432	62.627329
1906.989437	500.399398	62.632334
1906.213879	459.299672	62.637338
1905.481955	431.734293	62.642343
1904.585405	381.711184	62.647348
1904.356696	327.756610	62.652353
1903.533936	291.624288	62.657358
1902.660118	258.821153	62.662362
1902.207299	219.656217	62.667367
1901.204439	182.666533	62.672372
1900.762699	150.988774	62.677377
1899.771913	118.742252	62.682382
1898.936236	76.714902	62.687386
1897.944666	52.520302	62.692391
1897.022621	28.762543	62.697396
1896.389961	-7.277784	62.702401
1895.562643	-15.276870	62.707406
1894.922145	-18.899783	62.712410
1892.503609	13.092940	62.717415
1890.125303	52.624792	62.722420
1889.896070	41.187712	62.727425
1889.888893	59.730015	62.732430
1890.605453	52.375174	62.737434
1890.394117	53.012696	62.742439
1889.751312	51.676633	62.747444
1889.204999	48.475553	62.752449
1888.241273	53.742439	62.757454
1887.162239	63.892360	62.762458
1886.283926	57.342617	62.767463
1886.022043	65.524155	62.772468
1885.768682	54.571849	62.777473
1884.765988	64.170353	62.782478
1884.043349	63.769449	62.787482
1883.327633	66.571702	62.792487
1882.160478	69.701079	62.797492
1882.427733	61.242771	62.802497
1881.920347	66.290567	62.807502
1881.533596	62.121171	62.812506
1880.081849	69.729964	62.817511
1879.698888	69.156869	62.822516
1879.251790	67.475935	62.827521
1878.321881	65.773882	62.832526
1877.735998	66.608056	62.837530
1877.217320	61.420429	62.842535
1876.342901	67.105215	62.847540
1875.789803	65.554647	62.852545
1874.619423	69.312144	62.857550
1873.933590	62.987304	62.862554
1873.236340	62.145571	62.867559
1872.913486	63.838398	62.872564
1873.135468	58.011236	62.877569
1871.935051	62.525681	62.882574
1870.792710	68.011738	62.887578
1870.822713	68.164686	62.892583
1870.060507	69.350118	62.897588
1869.302329	66.305673	62.902593
1868.064476	67.254392	62.907598
1868.102611	60.682160	62.912602
1867.656515	55.673819	62.917607
1866.712319	62.049326	62.922612
1865.670574	61.976621	62.927617
1865.166225	79.307973	62.932622
1864.997594	63.814938	62.937626
1863.783327	63.294978	62.942631
1862.970890	66.626658	62.947636
1863.242991	67.565888	62.952641
1862.198657	70.833465	62.957646
1860.725691	75.436918	62.962650
1861.009902	73.570501	62.967655
1860.302633	63.749932	62.972660
1858.822264	62.807035	62.977665
1858.513271	62.827729	62.982670
1858.289728	59.020343	62.987674
1858.111646	69.057201	62.992679
1856.238536	76.690329	62.997684
1856.206375	68.400974	63.002689
1855.165096	64.630376	63.007694
1855.176130	61.798116	63.012698
1854.254416	66.578970	63.017703
1853.045019	64.416692	63.022708
1852.540808	62.946674	63.027713
1852.682597	70.978974	63.032718
1851.572473	69.557846	63.037722
1850.860818	70.807795	63.042727
1849.204121	69.121796	63.047732
1849.633198	57.942881	63.052737
1849.676562	72.675272	63.057742
1848.353139	64.841654	63.062746
1847.995246	64.357621	63.067751
1846.888821	67.338603	63.072756
1846.714643	73.345872	63.077761
1845.636380	72.231913	63.082766
1844.956161	71.297601	63.087770
1844.611965	71.839531	63.092775
1843.279997	68.941382	63.097780
1843.086886	65.706310	63.102785
1841.974627	71.987090	63.107790
1841.419134	66.185595	63.112794
1841.295811	66.049083	63.117799
1839.901971	72.986406	63.122804
1839.664214	59.044986	63.127809
1839.039179	67.826635	63.132814
1838.108591	70.664591	63.137818
1837.802033	59.602471	63.142823
1836.838104	66.949335	63.147828
1836.568932	58.946768	63.152833
1835.592828	72.316158	63.157838
1835.180006	63.066994	63.162842
1835.145680	58.688694	63.167847
1834.251853	73.650303	63.172852
1833.680751	54.233213	63.177857
1832.071090	72.378690	63.182862
1831.250857	59.814923	63.187866
1831.358817	59.993339	63.192871
1830.509064	69.154431	63.197876
1829.810643	55.489577	63.202881
1828.816916	67.647554	63.207886
1828.238272	56.581331	63.212890
1827.900802	68.758111	63.217895
1827.346876	68.130170	63.222900
1827.188488	53.980621	63.227905
1826.262784	61.351378	63.232910
1825.636448	70.950069	63.237914
1824.859547	74.249312	63.242919
1823.617910	71.571790	63.247924
1823.485672	60.713799	63.252929
1822.786564	76.746747	63.257934
1821.653672	69.139924	63.262938
1821.622334	66.457890	63.267943
1820.849973	70.374556	63.272948
1820.329644	60.543246	63.277953
1818.796783	67.018542	63.282958
1817.844928	71.190781	63.287962
1817.852103	68.606707	63.292967
1817.562715	77.611028	63.297972
1816.783575	56.389889	63.302977
1815.780411	72.412765	63.307982
1814.876846	71.846648	63.312986
1814.513500	67.315591	63.317991
1813.846552	80.700560	63.322996
1813.538648	66.784469	63.328001
1813.057318	75.007164	63.333006
1812.914128	63.971145	63.338010
1811.700877	76.269640	63.343015
1810.371119	74.225836	63.348020
1810.059905	57.877128	63.353025
1809.177228	74.215178	63.358030
1808.583282	70.291573	63.363034
1808.174255	72.201509	63.368039
1807.217200	73.791621	63.373044
1807.047221	70.401497	63.378049
1807.025325	73.314369	63.383054
1806.155533	62.075190	63.388058
1804.627862	67.759645	63.393063
1803.794392	78.605443	63.398068
1803.260564	69.429111	63.403073
1802.838196	67.950838	63.408078
1802.575674	80.437414	63.413082
1802.023416	65.618719	63.418087
1800.898483	69.832637	63.423092
1800.268507	67.084813	63.428097
1799.638679	65.983246	63.433102
1799.036454	70.935731	63.438106
1798.540408	77.282682	63.443111
1797.764383	78.236948	63.448116
1797.167910	66.404033	63.453121
1795.984014	72.352441	63.458126
1794.915275	72.940040	63.463130
1794.583618	60.885316	63.468135
1794.065350	65.488590	63.473140
1793.803804	56.626990	63.478145
1793.195916	75.170063	63.483150
1792.547384	69.506352	63.488154
1792.285282	70.194519	63.493159
1790.750417	71.463238	63.498164
1790.056686	64.671341	63.503169
1789.226487	68.204552	63.508174
1788.805788	64.261329	63.513178
1788.616032	69.112052	63.518183
1787.652382	74.057277	63.523188
1787.496757	65.117355	63.528193
1787.256686	72.849173	63.533198
1785.970255	73.890796	63.538202
1785.248803	57.537854	63.543207
1784.397818	62.769527	63.548212
1784.225769	77.477772	63.553217
1783.156738	68.072628	63.558222
1782.076595	63.086140	63.563226
1781.671504	63.500556	63.568231
1780.679930	69.175588	63.573236
1780.276736	64.857439	63.578241
1779.709941	73.443778	63.583246
1779.050417	62.149146	63.588250
1778.730509	60.946334	63.593255
1778.223571	69.606742	63.598260
1777.526541	62.933640	63.603265
1776.732341	67.981265	63.608270
1775.640919	71.455039	63.613274
1775.609402	61.601314	63.618279
1774.612456	58.697313	63.623284
1773.759317	66.045525	63.628289
1772.744789	63.693075	63.633294
1771.851061	64.180355	63.638298
1772.200756	65.389517	63.643303
1771.276457	67.447509	63.648308
1770.882734	58.143294	63.653313
1770.406840	62.079123	63.658318
1769.625305	66.643785	63.663322
1768.742118	59.271724	63.668327
1767.405136	68.166437	63.673332
1767.382831	66.113728	63.678337
1766.520845	61.447406	63.683342
1766.302674	60.291517	63.688346
1765.876448	66.692032	63.693351
1764.311996	62.878401	63.698356
1763.883933	54.667701	63.703361
1763.032957	59.457847	63.708366
1762.378450	59.949718	63.713370
1762.397652	58.407641	63.718375
1761.698626	66.690136	63.723380
1760.832981	56.432729	63.728385
1759.699598	63.380761	63.733390
1758.949948	57.638508	63.738394
1758.845413	55.870085	63.743399
1758.084015	68.558868	63.748404
1757.778200	59.748456	63.753409
1757.171692	57.164070	63.758414
1756.022140	66.279749	63.763418
1755.397431	62.695347	63.768423
1754.579223	63.285753	63.773428
1754.536558	61.630503	63.778433
1753.435849	55.817849	63.783438
1752.225170	65.611839	63.788442
1752.162973	55.018699	63.793447
1751.494235	64.720320	63.798452
1750.850427	57.784898	63.803457
1750.628372	54.470859	63.808462
1749.539065	64.989869	63.813466
1748.844397	51.226690	63.818471
1747.545574	61.633896	63.823476
1747.679640	63.178483	63.828481
1746.896124	58.506016	63.833486
1746.468722	53.724962	63.838490
1746.101114	57.787094	63.843495
1744.721348	65.332480	63.848500
1743.978712	57.786728	63.853505
1743.363359	65.587600	63.858510
1742.742468	53.195642	63.863514
1742.488744	50.031708	63.868519
1741.687503	61.695527	63.873524
1740.899167	52.569103	63.878529
1739.897170	64.528146	63.883534
1739.343607	55.173634	63.888538
1739.054246	58.163669	63.893543
1738.459037	64.684058	63.898548
1738.141608	56.756980	63.903553
1737.097464	58.652672	63.908558
1735.952395	58.738348	63.913562
1735.613283	53.222634	63.918567
1734.753745	65.029750	63.923572
1734.799941	50.548125	63.928577
1733.738744	59.676583	63.933582
1732.495689	58.502115	63.938586
1732.502487	52.133560	63.943591
1731.890739	60.142008	63.948596
1731.439646	47.825592	63.953601
1730.278352	56.406994	63.958606
1729.242929	56.984597	63.963610
1728.787387	51.424300	63.968615
1727.973829	56.388278	63.973620
1728.048996	62.012181	63.978625
1727.607338	61.519391	63.983630
1726.728861	58.598173	63.988634
1725.642417	57.602256	63.993639
1724.761874	61.558201	63.998644
1724.564997	56.820961	64.003649
1723.839680	66.693993	64.008654
1723.487316	56.446548	64.013658
1722.215310	59.507488	64.018663
1721.336003	64.729485	64.023668
1720.924920	59.575272	64.028673
1720.519644	58.673020	64.033678
1720.253836	58.344685	64.038682
1719.726544	60.257645	64.043687
1718.276211	75.697150	64.048692
1717.918575	63.517264	64.053697
1717.332920	58.182627	64.058702
1716.643144	58.998643	64.063706
1715.673373	55.322404	64.068711
1714.526185	60.747788	64.073716
1714.255919	60.978382	64.078721
1713.716351	69.718092	64.083726
1713.232861	63.085213	64.088730
1713.285030	63.155794	64.093735
1711.997565	63.062253	64.098740
1711.353882	70.503369	64.103745
1710.498972	64.959190	64.108750
1709.672350	74.966586	64.113754
1709.760258	57.542155	64.118759
1708.742919	67.606642	64.123764
1707.864386	62.463594	64.128769
1707.000407	65.101786	64.133774
1706.509683	69.464165	64.138778
1706.048725	64.144417	64.143783
1705.405048	67.890869	64.148788
1705.030785	59.830903	64.153793
1704.027122	70.350520	64.158798
1702.975588	69.536718	64.163802
1702.996317	57.593205	64.168807
1702.278155	63.626944	64.173812
1700.859032	70.569922	64.178817
1700.105896	64.375672	64.183822
1699.456599	60.525542	64.188826
1699.618863	60.901901	64.193831
1698.760762	67.134479	64.198836
1698.663942	53.744705	64.203841
1697.519485	68.288839	64.208846
1696.625403	63.824752	64.213850
1696.355640	62.103074	64.218855
1695.669374	68.319401	64.223860
1694.687627	61.264210	64.228865
1693.934329	63.443296	64.233870
1693.052699	60.648742	64.238874
1692.909830	57.397824	64.243879
1692.121983	60.373997	64.248884
1691.556482	52.623521	64.253889
1690.372031	71.939383	64.258894
1689.603819	73.143166	64.263898
1689.416823	61.587445	64.268903
1688.877158	62.542047	64.273908
1688.575661	58.605144	64.278913
1687.896760	63.036834	64.283918
1686.399919	61.224632	64.288922
1686.001491	56.932555	64.293927
1685.434010	62.157072	64.298932
1685.009286	62.301819	64.303937
1684.697673	58.795438	64.308942
1683.594533	66.817291	64.313946
1683.189453	60.812186	64.318951
1682.427304	67.177757	64.323956
1681.682681	49.478730	64.328961
1680.650017	54.494866	64.333966
1680.050345	63.181046	64.338970
1679.605222	49.531221	64.343975
1679.009965	60.851686	64.348980
1678.646939	60.100420	64.353985
1677.883344	68.694373	64.358990
1677.110404	70.332555	64.363994
1676.818042	55.698134	64.368999
1675.396864	69.871504	64.374004
1674.586580	59.162234	64.379009
1674.010662	62.953120	64.384014
1673.278575	66.084441	64.389018
1673.149147	54.921693	64.394023
1672.652552	63.389660	64.399028
1671.648570	63.560184	64.404033
1670.795899	64.930345	64.409038
1670.206000	55.144826	64.414042
1670.210368	52.457129	64.419047
1668.798715	55.404660	64.424052
1668.180800	58.886839	64.429057
1667.653354	64.434571	64.434062
1667.212545	55.489511	64.439066
1666.797297	59.994440	64.444071
1665.208412	61.957760	64.449076
1664.696699	62.937888	64.454081
1664.102708	55.665013	64.459086
1663.541210	55.686413	64.464090
1663.608958	53.242529	64.469095
1662.749074	56.919254	64.474100
1661.343706	57.290726	64.479105
1660.827742	57.900960	64.484110
1660.046046	58.663784	64.489114
1659.936081	52.192360	64.494119
1659.110322	60.718918	64.499124
1659.074772	61.371112	64.504129
1657.924823	59.877551	64.509134
1657.110257	59.538618	64.514138
1656.664650	56.050372	64.519143
1655.749428	62.897560	64.524148
1654.839071	61.138871	64.529153
1654.197440	52.203638	64.534158
1653.352116	66.824843	64.539162
1653.066612	53.056633	64.544167
1652.673383	60.284513	64.549172
1652.421414	61.541918	64.554177
1651.586677	48.958470	64.559182
1650.600879	58.450277	64.564186
1649.968786	51.861523	64.569191
1649.131878	55.632369	64.574196
1648.402914	49.880565	64.579201
1647.855048	62.257908	64.584206
1647.225773	51.418982	64.589210
1646.892553	56.557409	64.594215
1645.424909	60.855783	64.599220
1644.663158	50.780618	64.604225
1644.432125	60.706028	64.609230
1643.704786	61.223689	64.614234
1643.670252	61.583997	64.619239
1643.194647	56.416397	64.624244
1642.180125	50.519150	64.629249
1641.079665	51.260076	64.634254
1640.781966	58.493282	64.639258
1640.028698	57.338826	64.644263
1638.941932	72.753723	64.649268
1638.129659	55.445487	64.654273
1638.081698	52.554800	64.659278
1637.236915	57.807602	64.664282
1637.134833	56.187024	64.669287
1636.370947	62.456689	64.674292
1635.595528	52.673846	64.679297
1634.729204	57.674614	64.684302
1634.241391	61.114057	64.689306
1633.572981	56.257773	64.694311
1632.512160	64.730218	64.699316
1631.881019	59.306639	64.704321
1631.689058	56.016218	64.709326
1630.518164	54.929682	64.714330
1629.854189	50.213040	64.719335
1628.985386	62.750171	64.724340
1628.358134	58.910753	64.729345
1628.252928	56.445458	64.734350
1627.804044	45.022823	64.739354
1626.943812	53.908083	64.744359
1625.643920	52.733235	64.749364
1625.088693	57.146868	64.754369
1624.739528	51.129744	64.759374
1623.969810	64.475852	64.764378
1623.776769	53.523484	64.769383
1622.501962	70.270765	64.774388
1621.817706	57.841607	64.779393
1621.509898	51.269157	64.784398
1620.813740	61.848748	64.789402
1620.696751	56.755069	64.794407
1619.341918	60.054709	64.799412
1618.569620	47.549665	64.804417
1618.505136	56.664900	64.809422
1617.686674	65.680724	64.814426
1616.763433	62.087016	64.819431
1615.653619	69.231624	64.824436
1615.367388	56.064332	64.829441
1615.066314	57.316926	64.834446
1614.471134	60.860156	64.839450
1614.341346	54.056007	64.844455
1612.874877	58.332134	64.849460
1612.335979	62.296916	64.854465
1611.667164	59.457548	64.859470
1610.478910	56.987690	64.864474
1609.953913	50.459204	64.869479
1609.074279	54.137505	64.874484
1608.501986	54.706236	64.879489
1608.256008	51.973158	64.884494
1607.717931	60.308953	64.889498
1607.794355	53.371126	64.894503
1606.776285	60.691962	64.899508
1605.790566	56.259817	64.904513
1604.951509	56.235440	64.909518
1603.963668	63.108370	64.914522
1603.548252	60.700240	64.919527
1602.904485	56.601689	64.924532
1602.497476	61.327659	64.929537
1602.074857	57.422627	64.934542
1600.727713	59.899494	64.939546
1600.413426	55.764372	64.944551
1599.713965	62.815410	64.949556
1599.243733	59.666965	64.954561
1598.228085	53.479767	64.959566
1597.493070	57.300671	64.964570
1597.061753	50.454544	64.969575
1596.533532	60.062902	64.974580
1596.008611	57.845628	64.979585
1594.728276	52.928879	64.984590
1594.335600	55.219429	64.989594
1593.683251	56.739132	64.994599
1593.333062	55.498580	64.999604
1592.604074	51.468764	65.004609
1591.920679	52.859363	65.009614
1590.745739	49.095927	65.014618
1590.634619	44.461775	65.019623
1589.939644	56.583379	65.024628
1589.029029	62.075303	65.029633
1588.220479	54.469121	65.034638
1587.398008	59.273709	65.039642
1587.347142	57.706497	65.044647
1586.667499	58.418439	65.049652
1585.612710	68.840558	65.054657
1585.127034	48.194229	65.059662
1584.277757	66.947526	65.064666
1584.165320	51.899789	65.069671
1583.538073	61.396153	65.074676
1582.219732	56.507524	65.079681
1581.721640	49.725623	65.084686
1581.207628	61.481028	65.089690
1581.206026	52.937708	65.094695
1580.020905	52.323368	65.099700
1578.930256	53.838592	65.104705
1578.612227	51.724067	65.109710
1577.643479	54.158175	65.114714
1577.765960	64.937291	65.119719
1576.833470	67.688904	65.124724
1575.735988	56.627928	65.129729
1575.625378	59.928609	65.134734
1574.358775	69.250597	65.139738
1573.777038	63.240466	65.144743
1573.456967	60.512854	65.149748
1572.766412	55.515034	65.154753
1571.899149	50.111643	65.159758
1570.822752	60.543501	65.164762
1570.489744	53.221309	65.169767
1569.907103	58.536557	65.174772
1569.345285	58.375110	65.179777
1569.375015	50.153230	65.184782
1567.982090	61.024868	65.189786
1567.396560	52.112290	65.194791
1566.875943	67.126606	65.199796
1565.921541	57.878405	65.204801
1565.085962	61.638027	65.209806
1564.351575	62.909007	65.214810
1564.090401	51.044996	65.219815
1563.518826	56.391601	65.224820
1562.855731	55.170806	65.229825
1562.121334	59.578224	65.234830
1561.195926	57.965458	65.239834
1560.889457	58.878306	65.244839
1560.338452	61.007942	65.249844
1559.376951	55.756716	65.254849
1558.679915	55.719251	65.259854
1557.874021	47.461408	65.264858
1557.757334	51.302349	65.269863
1556.677433	59.139206	65.274868
1555.993379	49.382880	65.279873
1555.500504	50.976599	65.284878
1554.899485	46.371400	65.289882
1554.569719	39.160662	65.294887
1553.464954	48.091094	65.299892
1552.666470	49.132573	65.304897
1552.465062	49.771696	65.309902
1551.550399	43.145873	65.314906
1550.503336	49.709691	65.319911
1549.796940	48.405896	65.324916
1549.311038	46.914112	65.329921
1548.919678	36.232968	65.334926
1548.276315	51.766644	65.339930
1547.806158	43.803957	65.344935
1546.762726	45.529302	65.349940
1546.408676	42.870172	65.354945
1545.795723	57.648424	65.359950
1544.440735	56.077109	65.364954
1543.634787	43.063382	65.369959
1543.398181	41.820561	65.374964
1542.882982	49.378470	65.379969
1542.658276	42.518456	65.384974
1542.025877	46.449218	65.389978
1540.988732	47.400891	65.394983
1540.581445	42.891067	65.399988
1539.551417	56.037274	65.404993
1538.606450	40.226159	65.409998
1537.853853	61.231660	65.415002
1537.895490	39.306300	65.420007
1537.207507	52.398159	65.425012
1536.496791	55.259621	65.430017
1535.600730	43.570610	65.435022
1534.512442	48.239254	65.440026
1534.367472	40.973928	65.445031
1534.135742	46.640261	65.450036
1533.454344	52.885800	65.455041
1532.600561	44.807458	65.460046
1531.704634	60.876417	65.465050
1531.428280	41.081498	65.470055
1530.474116	54.180961	65.475060
1529.646334	45.828840	65.480065
1529.477481	46.833361	65.485070
1528.013863	50.000523	65.490074
1527.421343	38.905084	65.495079
1526.811878	51.626515	65.500084
1526.300220	45.846535	65.505089
1526.281196	52.535590	65.510094
1524.909692	45.250687	65.515098
1524.392228	48.278557	65.520103
1523.940129	44.103849	65.525108
1523.224513	44.564490	65.530113
1522.272772	48.493958	65.535118
1521.152957	60.757190	65.540122
1520.776686	42.227047	65.545127
1520.557566	51.778409	65.550132
1520.391863	44.305075	65.555137
1519.531742	47.813149	65.560142
1518.336949	48.996452	65.565146
1517.988277	37.059637	65.570151
1517.161722	49.916481	65.575156
1516.346296	60.811494	65.580161
1515.745395	46.358610	65.585166
1515.015161	45.454412	65.590170
1514.883151	50.228152	65.595175
1513.935537	44.268298	65.600180
1513.036135	43.446172	65.605185
1512.760062	48.722176	65.610190
1511.779722	48.318171	65.615194
1511.285446	56.613901	65.620199
1510.380863	45.053982	65.625204
1509.659984	48.010101	65.630209
1509.393205	42.937085	65.635214
1508.425599	49.333756	65.640218
1508.777598	37.987325	65.645223
1507.554547	49.243555	65.650228
1506.748515	47.230236	65.655233
1505.803820	43.136958	65.660238
1504.436739	51.793712	65.665242
1504.120899	40.416207	65.670247
1503.672620	49.787947	65.675252
1503.269287	38.832760	65.680257
1503.300566	39.414413	65.685262
1501.827625	53.402103	65.690266
1501.335031	44.933659	65.695271
1500.357773	59.213161	65.700276
1500.164319	62.804539	65.705281
1499.726282	43.648729	65.710286
1498.821907	56.084303	65.715290
1497.999355	50.021006	65.720295
1497.479135	50.549949	65.725300
1496.621269	48.994283	65.730305
1495.703133	58.115849	65.735310
1494.770501	57.571811	65.740314
1494.625438	55.475543	65.745319
1494.167060	42.351419	65.750324
1493.907049	56.846519	65.755329
1493.029661	45.200289	65.760334
1491.982447	57.619141	65.765338
1491.657024	53.982528	65.770343
1490.694578	53.987256	65.775348
1490.041081	59.222318	65.780353
1489.302308	52.849254	65.785358
1488.692180	51.935440	65.790362
1488.427541	50.506276	65.795367
1487.486389	41.853658	65.800372
1486.528723	44.584067	65.805377
1486.239756	45.282838	65.810382
1485.687682	48.858663	65.815386
1484.595853	53.280318	65.820391
1483.989274	51.363040	65.825396
1483.557099	44.495004	65.830401
1483.089154	51.506116	65.835406
1482.400428	58.686350	65.840410
1481.639065	44.421399	65.845415
1480.988118	44.616319	65.850420
1480.290085	38.000258	65.855425
1479.201117	53.658365	65.860430
1478.739616	48.445990	65.865434
1478.348883	49.526771	65.870439
1477.677988	53.296515	65.875444
1477.086706	53.060925	65.880449
1475.907898	43.604018	65.885454
1475.321629	55.632671	65.890458
1474.983839	47.221631	65.895463
1474.716204	54.713403	65.900468
1473.566195	49.413328	65.905473
1472.822694	46.615831	65.910478
1472.135452	57.206640	65.915482
1471.674169	45.497452	65.920487
1470.519756	44.427294	65.925492
1469.884428	57.632219	65.930497
1469.691603	52.269921	65.935502
1468.905907	56.373288	65.940506
1468.985752	42.282162	65.945511
1467.824736	50.631807	65.950516
1467.052847	51.197595	65.955521
1466.758847	43.456086	65.960526
1465.465648	54.253569	65.965530
1464.816340	45.258127	65.970535
1464.186888	42.153940	65.975540
1463.744735	52.360461	65.980545
1463.017904	46.092741	65.985550
1461.933969	59.291690	65.990554
1461.573567	47.358322	65.995559
1460.925375	57.167098	66.000564
1460.654237	49.538644	66.005569
1460.136963	42.714098	66.010574
1458.734270	50.808850	66.015578
1458.393157	35.712344	66.020583
1457.978466	49.610722	66.025588
1457.159695	48.730073	66.030593
1456.131764	44.743078	66.035598
1455.401535	45.545090	66.040602
1455.210723	48.949975	66.045607
1454.647667	49.504656	66.050612
1453.738401	57.388543	66.055617
1452.905712	50.964189	66.060622
1452.218111	53.564965	66.065626
1452.058666	57.202977	66.070631
1451.102638	47.898327	66.075636
1450.525086	48.116282	66.080641
1450.077896	47.414694	66.085646
1449.165632	68.567005	66.090650
1448.618542	47.449543	66.095655
1447.703286	57.647678	66.100660
1446.777180	65.067488	66.105665
1446.543462	46.055836	66.110670
1445.919894	49.668260	66.115674
1444.899480	48.062753	66.120679
1444.150052	56.958833	66.125684
1443.589452	47.659152	66.130689
1443.529829	47.041048	66.135694
1442.954523	55.065820	66.140698
1442.195824	46.398417	66.145703
1441.356956	48.203253	66.150708
1440.472247	43.815052	66.155713
1440.290555	47.073413	66.160718
1439.063293	45.155443	66.165722
1438.824607	38.032753	66.170727
1438.162648	48.395625	66.175732
1436.965672	42.164786	66.180737
1436.465457	31.953542	66.185742
1435.644810	45.889625	66.190746
1435.460800	55.151569	66.195751
1434.954032	56.116761	66.200756
1433.789531	43.510135	66.205761
1433.359046	45.483450	66.210766
1432.602493	51.007700	66.215770
1432.259146	38.155465	66.220775
1431.255052	39.258040	66.225780
1430.529741	56.991896	66.230785
1430.396032	45.236968	66.235790
1429.207367	51.938443	66.240794
1428.466743	36.462332	66.245799
1428.115052	47.430303	66.250804
1427.294827	60.180515	66.255809
1427.280140	43.571933	66.260814
1425.888252	52.538580	66.265818
1425.509583	43.626292	66.270823
1424.833648	51.077302	66.275828
1423.581801	45.072801	66.280833
1422.986847	36.488193	66.285838
1422.281703	46.052140	66.290842
1421.969341	45.196671	66.295847
1421.873445	46.847165	66.300852
1421.216585	50.225198	66.305857
1420.259442	42.314712	66.310862
1419.316011	49.601663	66.315866
1419.054227	35.985873	66.320871
1418.044300	47.312336	66.325876
1417.090249	40.330148	66.330881
1416.720046	37.227349	66.335886
1416.230186	44.920009	66.340890
1415.765529	32.410326	66.345895
1414.286627	44.427884	66.350900
1413.583852	43.647080	66.355905
1413.727577	41.228968	66.360910
1412.939937	54.335106	66.365914
1412.626878	43.408169	66.370919
1411.423488	38.551834	66.375924
1410.882013	38.297306	66.380929
1410.559518	41.054519	66.385934
1409.051245	47.439382	66.390938
1408.452128	40.918006	66.395943
1408.280817	44.630438	66.400948
1407.725971	36.135651	66.405953
1407.337057	39.721824	66.410958
1406.109148	41.706768	66.415962
1405.295075	39.751529	66.420967
1405.126054	43.099337	66.425972
1404.264452	43.731439	66.430977
1403.633103	42.060960	66.435982
1402.458863	49.572249	66.440986
1402.138858	47.965822	66.445991
1401.950323	47.409206	66.450996
1400.815669	48.898381	66.456001
1400.051090	47.014122	66.461006
1399.451430	50.673215	66.466010
1398.986443	49.908236	66.471015
1398.559464	46.732464	66.476020
1397.702659	42.018160	66.481025
1396.917218	33.331380	66.486030
1396.237825	52.431402	66.491034
1396.225409	43.550792	66.496039
1395.200842	45.692649	66.501044
1394.401508	49.399249	66.506049
1394.173728	47.568439	66.511054
1392.671916	48.152495	66.516058
1392.290102	50.343576	66.521063
1392.001772	41.074755	66.526068
1390.986950	44.616916	66.531073
1389.975515	43.658106	66.536078
1389.448175	50.629784	66.541082
1388.992749	48.447242	66.546087
1388.142510	45.650969	66.551092
1387.933197	46.851155	66.556097
1387.599620	39.823976	66.561102
1386.403365	48.043637	66.566106
1386.156922	45.995031	66.571111
1385.234244	50.082344	66.576116
1383.864269	46.939767	66.581121
1383.450418	41.300392	66.586126
1382.691465	44.052867	66.591130
1382.697571	35.625040	66.596135
1382.185619	40.399244	66.601140
1381.189783	38.217449	66.606145
1380.933320	42.687706	66.611150
1379.414695	42.309387	66.616154
1378.716212	44.593378	66.621159
1378.143763	25.140472	66.626164
1377.463981	41.867333	66.631169
1377.090806	27.933389	66.636174
1376.758576	40.601298	66.641178
1376.087376	31.319229	66.646183
1375.252826	38.964179	66.651188
1374.673661	35.907216	66.656193
1374.407801	30.458782	66.661198
1372.765768	41.762726	66.666202
1372.102778	31.847022	66.671207
1371.855536	32.908163	66.676212
1371.212152	43.498313	66.681217
1371.088362	32.921341	66.686222
1369.704312	41.401079	66.691226
1369.178471	26.384432	66.696231
1368.535640	36.156087	66.701236
1367.902880	36.870093	66.706241
1367.105748	35.620197	66.711246
1366.368507	49.617151	66.716250
1365.697653	34.309747	66.721255
1365.532423	23.930171	66.726260
1365.081672	47.013323	66.731265
1364.095902	31.626673	66.736270
1363.447932	40.542900	66.741274
1362.834604	29.824556	66.746279
1362.033174	41.327614	66.751284
1361.224403	42.269863	66.756289
1360.764546	43.842598	66.761294
1359.946492	43.986843	66.766298
1358.861384	40.341704	66.771303
1358.533257	40.039083	66.776308
1357.815378	39.642302	66.781313
1357.772791	38.677731	66.786318
1356.784240	44.937433	66.791322
1355.889544	44.108307	66.796327
1355.419324	49.635944	66.801332
1354.923903	43.768277	66.806337
1354.398263	42.167737	66.811342
1353.078505	49.546063	66.816346
1352.586253	41.369333	66.821351
1352.540959	40.789952	66.826356
1351.402833	40.097290	66.831361
1350.859974	54.071237	66.836366
1350.250500	47.515254	66.841370
1349.599823	45.136686	66.846375
1348.461777	31.346405	66.851380
1347.486930	44.830794	66.856385
1347.697287	39.264086	66.861390
1346.965139	38.264053	66.866394
1346.418775	35.884675	66.871399
1345.479231	49.194730	66.876404
1344.323102	45.502541	66.881409
1344.368431	28.460270	66.886414
1343.371212	53.576170	66.891418
1342.516115	39.356148	66.896423
1342.121535	43.129303	66.901428
1341.396620	44.226955	66.906433
1341.264707	34.226841	66.911438
1340.339681	44.801845	66.916442
1339.585875	46.312504	66.921447
1339.343067	40.122425	66.926452
1338.107116	50.868278	66.931457
1337.483759	41.884527	66.936462
1336.415292	56.050832	66.941466
1335.963060	46.196242	66.946471
1335.804760	42.722318	66.951476
1334.743044	47.298507	66.956481
1334.168489	41.233700	66.961486
1333.447081	45.755792	66.966490
1333.077253	36.850010	66.971495
1332.824628	46.793028	66.976500
1331.473339	47.728491	66.981505
1331.208438	32.280881	66.986510
1330.639210	54.105599	66.991514
1329.467333	41.001913	66.996519
1328.937324	38.733474	67.001524
1327.917407	48.215017	67.006529
1327.720973	39.953425	67.011534
1326.781761	35.602319	67.016538
1325.784307	47.011975	67.021543
1325.496763	38.626101	67.026548
1325.104971	41.965171	67.031553
1324.876096	41.966884	67.036558
1323.400851	51.768383	67.041562
1322.734073	41.758679	67.046567
1322.456950	54.149768	67.051572
1321.751059	49.504537	67.056577
1321.278469	42.688696	67.061582
1320.648767	45.294489	67.066586
1319.803759	42.645637	67.071591
1319.466830	50.864332	67.076596
1318.155726	38.818802	67.081601
1317.496430	41.676871	67.086606
1317.037902	42.076199	67.091610
1316.524466	37.073965	67.096615
1315.220697	39.979294	67.101620
1314.555782	43.316053	67.106625
1314.090413	40.466510	67.111630
1313.814942	54.096767	67.116634
1313.550162	36.660685	67.121639
1313.042216	32.652595	67.126644
1311.996187	47.800884	67.131649
1311.573791	43.667232	67.136654
1310.281106	36.045098	67.141658
1309.542925	38.910978	67.146663
1309.173985	41.148905	67.151668
1308.424005	48.269521	67.156673
1308.182957	50.651114	67.161678
1307.451006	50.288122	67.166682
1306.811645	40.365526	67.171687
1305.791591	42.248089	67.176692
1304.820457	43.744424	67.181697
1304.480603	42.199512	67.186702
1303.863056	40.753937	67.191706
1303.446816	39.719464	67.196711
1302.808591	43.591277	67.201716
1301.958123	55.576795	67.206721
1301.739617	36.211137	67.211726
1300.518795	43.745635	67.216730
1299.723598	43.870496	67.221735
1299.228520	37.788335	67.226740
1298.376358	42.463680	67.231745
1297.608758	41.679022	67.236750
1296.829807	47.569546	67.241754
1296.254699	49.395570	67.246759
1295.827111	37.715777	67.251764
1295.402358	45.899548	67.256769
1294.967043	37.258065	67.261774
1293.941989	37.556659	67.266778
1293.101902	42.569115	67.271783
1293.104223	28.725305	67.276788
1291.544543	41.220937	67.281793
1291.071569	34.525011	67.286798
1290.240235	34.352858	67.291802
1289.890791	35.624211	67.296807
1290.149073	40.941423	67.301812
1288.969646	36.705789	67.306817
1287.816077	39.145725	67.311822
1287.157339	41.376113	67.316826
1286.828556	42.946944	67.321831
1286.257918	40.541477	67.326836
1285.203552	46.947278	67.331841
1284.928484	40.230926	67.336846
1283.957202	34.740119	67.341850
1282.951251	46.482282	67.346855
1282.844415	32.643208	67.351860
1282.017639	34.312133	67.356865
1281.755025	44.042281	67.361870
1280.621334	40.613051	67.366874
1280.076729	40.303857	67.371879
1279.494605	34.904140	67.376884
1278.701567	43.710987	67.381889
1278.164298	39.111503	67.386894
1277.291971	40.469142	67.391898
1276.761856	43.620482	67.396903
1276.462912	39.038299	67.401908
1275.170799	45.297405	67.406913
1274.636708	50.149262	67.411918
1274.134964	44.396156	67.416922
1273.526405	53.692476	67.421927
1273.111922	53.233291	67.426932
1272.136093	42.372339	67.431937
1271.850577	41.615119	67.436942
1271.003786	40.265921	67.441946
1269.991577	45.528090	67.446951
1269.236596	50.019268	67.451956
1268.614304	42.995438	67.456961
1268.232369	43.410982	67.461966
1267.653913	35.008298	67.466970
1266.919624	45.327500	67.471975
1266.416593	40.948069	67.476980
1265.600774	45.365344	67.481985
1265.035853	41.864616	67.486990
1264.135071	43.726656	67.491994
1263.358177	48.643923	67.496999
1263.440104	39.910750	67.502004
1262.160539	44.682441	67.507009
1261.716174	39.385400	67.512014
1261.135440	45.624446	67.517018
1260.054478	36.257760	67.522023
1259.441624	38.531318	67.527028
1258.351381	43.867396	67.532033
1258.298638	42.855559	67.537038
1257.372938	43.523131	67.542042
1257.221378	47.316002	67.547047
1256.436631	41.276752	67.552052
1255.530938	40.756903	67.557057
1255.101036	45.161707	67.562062
1254.597323	42.501190	67.567066
1253.662194	45.106676	67.572071
1253.009932	40.249526	67.577076
1252.049912	46.525225	67.582081
1252.035666	36.110617	67.587086
1250.998042	46.031794	67.592090
1250.070275	46.190363	67.597095
1249.912624	38.168612	67.602100
1248.955217	53.522019	67.607105
1248.378352	42.832601	67.612110
1247.168381	51.980128	67.617114
1247.026636	39.061199	67.622119
1246.882718	46.154849	67.627124
1245.521899	42.370681	67.632129
1244.657107	43.151570	67.637134
1244.365445	50.555706	67.642138
1243.709170	47.512612	67.647143
1243.808982	38.910631	67.652148
1242.659325	46.523721	67.657153
1242.068635	37.624693	67.662158
1241.148774	40.137872	67.667162
1239.890975	39.491095	67.672167
1239.518725	27.211198	67.677172
1238.690472	43.897026	67.682177
1238.697500	32.212803	67.687182
1238.624808	45.339320	67.692186
1237.137588	43.716662	67.697191
1236.556912	40.734088	67.702196
1235.920271	49.484543	67.707201
1235.184784	38.963849	67.712206
1234.568164	44.634619	67.717210
1233.623603	42.542498	67.722215
1233.443603	46.740420	67.727220
1232.335842	49.829082	67.732225
1231.812195	44.060548	67.737230
1231.144718	51.888700	67.742234
1230.285640	50.959343	67.747239
1230.026769	35.349957	67.752244
1229.106023	49.234187	67.757249
1228.494585	48.331684	67.762254
1227.800948	52.477243	67.767258
1227.513717	41.457941	67.772263
1226.691264	39.557710	67.777268
1225.670265	54.296788	67.782273
1225.165048	41.076125	67.787278
1225.065333	40.667820	67.792282
1224.172858	51.392215	67.797287
1223.511235	33.688118	67.802292
1222.698795	46.992179	67.807297
1221.829470	42.475468	67.812302
1221.167628	52.363713	67.817306
1220.670752	42.008501	67.822311
1220.221926	51.724109	67.827316
1219.345446	41.974858	67.832321
1218.298652	53.159014	67.837326
1217.739472	53.019300	67.842330
1217.115322	51.024464	67.847335
1216.808121	42.435164	67.852340
1216.163375	53.697311	67.857345
1215.390013	48.099368	67.862350
1214.655748	42.086798	67.867354
1214.278651	53.971832	67.872359
1213.713281	37.233252	67.877364
1212.560161	49.233792	67.882369
1212.134988	47.295623	67.887374
1211.435014	35.165605	67.892378
1210.133319	49.436828	67.897383
1210.136264	44.559081	67.902388
1209.446531	50.358173	67.907393
1209.241807	37.586456	67.912398
1207.972721	48.911609	67.917402
1207.043077	47.400572	67.922407
1206.690025	48.886966	67.927412
1206.164363	48.178979	67.932417
1205.740741	40.205833	67.937422
1204.692279	49.121121	67.942426
1204.237218	43.598720	67.947431
1203.799037	47.790391	67.952436
1202.789683	40.807632	67.957441
1201.863833	53.412254	67.962446
1201.825940	39.218467	67.967450
1201.008044	46.742549	67.972455
1200.207775	49.233572	67.977460
1199.265192	39.550035	67.982465
1199.036003	49.013108	67.987470
1198.609981	46.567320	67.992474
1197.177691	57.705557	67.997479
1196.899638	43.401728	68.002484
1196.107527	42.854378	68.007489
1195.814778	40.915656	68.012494
1194.798839	50.809751	68.017498
1193.694353	51.882650	68.022503
1193.672953	38.703332	68.027508
1193.247676	53.724562	68.032513
1192.536866	50.732730	68.037518
1191.615085	36.848227	68.042522
1190.498963	47.543538	68.047527
1190.396191	40.664194	68.052532
1189.453378	55.573767	68.057537
1188.613531	46.329613	68.062542
1188.123004	47.582415	68.067546
1187.823477	48.511544	68.072551
1187.140531	34.294189	68.077556
1185.673143	53.606259	68.082561
1185.321431	46.336009	68.087566
1185.137260	52.616082	68.092570
1184.614869	48.315438	68.097575
1184.082315	42.702869	68.102580
1182.497001	45.145277	68.107585
1182.408162	34.496548	68.112590
1182.116054	47.725758	68.117594
1180.660914	40.514291	68.122599
1180.392938	38.847586	68.127604
1179.466926	51.305587	68.132609
1179.040064	39.084842	68.137614
1178.527175	50.750205	68.142618
1177.557910	36.538961	68.147623
1177.683321	51.597191	68.152628
1176.256988	50.944131	68.157633
1175.609909	53.647334	68.162638
1175.000007	42.114832	68.167642
1174.232783	47.375920	68.172647
1174.194144	43.611760	68.177652
1172.869504	50.473723	68.182657
1172.433931	44.673853	68.187662
1171.461969	42.661804	68.192666
1171.094017	45.817336	68.197671
1170.928613	39.163988	68.202676
1169.483466	44.843530	68.207681
1169.190791	34.216180	68.212686
1168.862217	42.085056	68.217690
1167.701624	47.408703	68.222695
1166.932091	43.852233	68.227700
1166.353008	47.572751	68.232705
1166.047215	38.264183	68.237710
1165.264397	46.804514	68.242714
1164.097473	44.438713	68.247719
1163.926887	44.412248	68.252724
1163.113008	53.616660	68.257729
1162.795868	43.564028	68.262734
1162.004885	45.318757	68.267738
1161.388791	58.113819	68.272743
1160.968888	51.526169	68.277748
1159.918971	52.022726	68.282753
1159.023188	46.735996	68.287758
1158.836533	42.598001	68.292762
1157.653545	44.232155	68.297767
1156.816456	43.483822	68.302772
1155.851592	43.880126	68.307777
1155.651238	49.984585	68.312782
1155.547929	49.529548	68.317786
1155.187333	48.412137	68.322791
1154.157726	43.575605	68.327796
1153.355481	42.047483	68.332801
1152.860781	43.006077	68.337806
1151.637011	41.532377	68.342810
1150.816760	48.124909	68.347815
1150.496532	41.557682	68.352820
1149.860844	51.320358	68.357825
1149.725167	38.033071	68.362830
1148.698084	44.904488	68.367834
1147.815949	41.946226	68.372839
1147.642488	41.355696	68.377844
1146.660437	48.089073	68.382849
1145.907633	44.736522	68.387854
1144.968142	42.075952	68.392858
1144.495619	55.270784	68.397863
1144.475673	44.235799	68.402868
1143.260472	42.886890	68.407873
1142.649870	53.675283	68.412878
1141.904098	49.600977	68.417882
1141.590090	50.347920	68.422887
1141.307825	46.316591	68.427892
1139.912011	51.354397	68.432897
1139.523734	54.495822	68.437902
1138.927950	49.664413	68.442906
1137.907514	37.922841	68.447911
1137.314396	47.006994	68.452916
1136.577383	45.175203	68.457921
1136.245596	51.221721	68.462926
1135.333421	35.738338	68.467930
1134.764896	55.219695	68.472935
1134.445007	37.677318	68.477940
1133.499665	52.664569	68.482945
1132.524925	47.855587	68.487950
1132.212433	49.431729	68.492954
1131.609009	46.323495	68.497959
1131.259845	32.313266	68.502964
1129.965808	49.118924	68.507969
1129.227153	44.885804	68.512974
1128.967411	51.315085	68.517978
1128.166466	43.091322	68.522983
1127.195942	50.513548	68.527988
1126.512582	41.717600	68.532993
1126.384672	47.633925	68.537998
1125.874108	38.747422	68.543002
1125.035443	49.963153	68.548007
1124.328857	45.439518	68.553012
1123.482346	53.088016	68.558017
1122.805745	39.648654	68.563022
1121.830113	52.392092	68.568026
1121.330795	43.816022	68.573031
1121.099772	38.306894	68.578036
1120.536812	42.020125	68.583041
1119.849584	48.416474	68.588046
1118.966543	45.876240	68.593050
1117.872084	61.760812	68.598055
1118.077818	41.641784	68.603060
1116.935462	54.630929	68.608065
1115.837928	40.553650	68.613070
1115.661152	35.767570	68.618074
1115.121466	51.887158	68.623079
1114.183183	37.201109	68.628084
1113.321105	48.116226	68.633089
1113.271479	55.458220	68.638094
1112.742234	45.256414	68.643098
1111.729064	45.695110	68.648103
1111.006691	47.254447	68.653108
1110.355539	57.215125	68.658113
1109.667749	45.362310	68.663118
1108.941487	48.500725	68.668122
1107.926237	53.988930	68.673127
1107.619819	42.118037	68.678132
1107.315062	59.280432	68.683137
1106.843784	51.603455	68.688142
1105.726932	57.640808	68.693146
1104.778657	60.048173	68.698151
1104.825453	45.024102	68.703156
1103.782698	55.734585	68.708161
1102.800585	53.757291	68.713166
1102.742623	50.228008	68.718170
1101.655797	39.277570	68.723175
1100.489974	52.150607	68.728180
1099.512314	48.411230	68.733185
1099.137374	47.600448	68.738190
1099.038713	48.210646	68.743194
1098.637008	45.272177	68.748199
1098.505691	47.729367	68.753204
1097.602104	46.218959	68.758209
1096.419169	52.903884	68.763214
1096.404437	38.931926	68.768218
1095.109782	59.025500	68.773223
1094.906591	34.920515	68.778228
1093.995991	54.587162	68.783233
1093.035910	52.737249	68.788238
1092.068018	46.031784	68.793242
1091.636201	43.594825	68.798247
1091.533511	29.904936	68.803252
1090.675164	55.175388	68.808257
1089.779115	49.123940	68.813262
1089.097495	57.153056	68.818266
1088.358879	55.671601	68.823271
1087.924555	48.390859	68.828276
1086.568868	42.319488	68.833281
1086.034936	51.747457	68.838286
1086.046676	42.822040	68.843290
1085.642270	53.932440	68.848295
1085.292517	40.378030	68.853300
1084.026376	36.600973	68.858305
1083.059337	49.111250	68.863310
1082.798372	48.864211	68.868314
1081.679623	50.650600	68.873319
1080.880182	51.085272	68.878324
1080.448088	47.885148	68.883329
1080.300224	45.133377	68.888334
1079.791532	39.859225	68.893338
1078.605713	46.817413	68.898343
1078.206080	33.411288	68.903348
1077.290238	42.012216	68.908353
1076.353881	46.451870	68.913358
1075.830689	55.748830	68.918362
1074.842721	54.907834	68.923367
1074.945386	51.086510	68.928372
1074.510510	54.602767	68.933377
1073.235080	48.971201	68.938382
1072.941026	36.423450	68.943386
1072.147454	45.979445	68.948391
1071.365577	40.914320	68.953396
1070.693182	48.710167	68.958401
1070.269914	40.845805	68.963406
1069.599156	32.563519	68.968410
1068.319581	47.506176	68.973415
1068.074911	39.310645	68.978420
1067.655480	49.146160	68.983425
1066.722047	35.649912	68.988430
1065.834601	36.593727	68.993434
1065.058418	45.221329	68.998439
1064.863991	35.740536	69.003444
1064.265088	38.603247	69.008449
1063.493763	36.791129	69.013454
1062.713710	42.025900	69.018458
1062.116924	36.130284	69.023463
1061.860025	37.205602	69.028468
1060.571233	40.249014	69.033473
1059.894425	40.586918	69.038478
1059.567830	47.086755	69.043482
1059.084831	41.961478	69.048487
1058.111354	42.228308	69.053492
1057.191093	54.018404	69.058497
1056.671725	40.934086	69.063502
1056.770545	36.733349	69.068506
1055.678516	44.119729	69.073511
1055.022516	44.504785	69.078516
1054.401417	40.249839	69.083521
1053.541375	47.410093	69.088526
1052.465362	44.790199	69.093530
1052.086545	42.630232	69.098535
1051.635031	39.311784	69.103540
1050.731166	53.532399	69.108545
1050.304650	38.315564	69.113550
1049.846779	47.111722	69.118554
1049.029881	48.307661	69.123559
1048.717382	39.052221	69.128564
1047.375977	49.654113	69.133569
1046.693943	45.642238	69.138574
1046.352878	41.959308	69.143578
1045.600232	47.863053	69.148583
1044.841132	43.145959	69.153588
1044.083518	43.605527	69.158593
1043.578678	41.358381	69.163598
1043.436153	34.906406	69.168602
1042.162044	49.356219	69.173607
1041.849580	43.164652	69.178612
1041.239147	51.283370	69.183617
1039.881154	46.319363	69.188622
1039.398619	45.544629	69.193626
1038.547042	51.768453	69.198631
1038.169199	35.826401	69.203636
1037.804412	45.238503	69.208641
1037.501800	43.302948	69.213646
1036.441357	41.398065	69.218650
1035.310840	43.041271	69.223655
1035.383336	45.314659	69.228660
1034.477396	46.766030	69.233665
1033.370559	39.139724	69.238670
1033.061810	42.189663	69.243674
1032.219699	40.314702	69.248679
1032.401335	38.595414	69.253684
1031.381471	45.752714	69.258689
1030.619689	38.418432	69.263694
1029.944931	43.913992	69.268698
1028.419056	48.652437	69.273703
1028.228384	44.075146	69.278708
1027.354375	42.970048	69.283713
1026.876438	43.951229	69.288718
1027.024119	45.443139	69.293722
1026.287634	51.752731	69.298727
1025.519958	46.592327	69.303732
1024.400874	31.048887	69.308737
1023.132522	46.935901	69.313742
1022.899418	45.454470	69.318746
1022.226673	40.539152	69.323751
1022.018261	39.977844	69.328756
1021.780241	37.292460	69.333761
1020.524278	49.282615	69.338766
1020.034754	45.599653	69.343770
1019.376915	47.795269	69.348775
1018.791311	50.594378	69.353780
1017.534927	53.990609	69.358785
1016.850997	40.714875	69.363790
1016.882456	40.238405	69.368794
1015.899437	49.237953	69.373799
1015.250665	48.853928	69.378804
1014.633426	38.407549	69.383809
1013.983489	44.126235	69.388814
1013.098046	37.609534	69.393818
1012.230819	49.249280	69.398823
1011.877327	43.507350	69.403828
1011.499713	39.696206	69.408833
1010.524782	41.445553	69.413838
1010.020241	45.734532	69.418842
1009.237130	46.172937	69.423847
1008.858144	45.069513	69.428852
1008.020626	36.462132	69.433857
1007.283612	37.546031	69.438862
1006.783161	47.400745	69.443866
1006.193553	41.511886	69.448871
1005.629134	50.006470	69.453876
1004.623892	47.673368	69.458881
1004.119408	47.581768	69.463886
1003.372500	38.961549	69.468890
1002.254532	47.350241	69.473895
1001.929609	46.577247	69.478900
1001.668860	46.238723	69.483905
1000.841445	49.590368	69.488910
999.769281	45.479733	69.493914
999.026043	47.408256	69.498919
998.984100	41.312427	69.503924
998.466458	43.879963	69.508929
997.140585	48.383188	69.513934
996.665329	31.863745	69.518938
995.864154	51.134541	69.523943
995.717624	49.593610	69.528948
994.414151	38.122637	69.533953
993.857265	52.582936	69.538958
993.435875	41.619725	69.543962
992.845014	47.606548	69.548967
992.619919	46.431337	69.553972
991.560238	50.083276	69.558977
990.898795	56.712085	69.563982
990.321791	39.866639	69.568986
988.878331	48.349696	69.573991
988.730735	31.128453	69.578996
988.156575	45.217773	69.584001
987.782474	42.364816	69.589006
987.100127	42.992191	69.594010
985.701891	44.193910	69.599015
985.589506	40.999709	69.604020
985.038705	39.494714	69.609025
983.666573	54.332290	69.614030
983.277365	37.922151	69.619034
982.299204	54.143044	69.624039
982.346090	44.494563	69.629044
981.867018	46.816281	69.634049
981.039740	53.851502	69.639054
980.357538	31.440652	69.644058
979.496797	52.725141	69.649063
979.302901	32.742263	69.654068
978.002788	41.760730	69.659073
977.484026	43.674043	69.664078
977.012014	45.214083	69.669082
976.596047	48.364661	69.674087
975.781277	30.314481	69.679092
975.106047	44.970213	69.684097
974.297197	43.304436	69.689102
973.540620	40.931785	69.694106
971.948125	54.246469	69.699111
971.951978	32.543293	69.704116
971.738249	43.246478	69.709121
971.249872	40.564664	69.714126
970.911178	29.250859	69.719130
969.463338	49.007723	69.724135
969.082339	41.852565	69.729140
968.564843	41.282094	69.734145
967.501145	35.235301	69.739150
967.037209	38.805076	69.744154
966.375537	36.690128	69.749159
966.191958	41.893096	69.754164
964.905914	46.468842	69.759169
964.329307	42.170575	69.764174
964.150877	37.720651	69.769178
962.780691	49.309551	69.774183
961.959579	42.232303	69.779188
961.497858	44.947060	69.784193
960.960035	39.994525	69.789198
961.189368	38.783284	69.794202
959.936853	55.043104	69.799207
959.356527	36.635515	69.804212
958.685290	45.363131	69.809217
957.424980	43.188899	69.814222
956.975190	45.151164	69.819226
956.227971	44.194643	69.824231
956.015286	38.521782	69.829236
955.041064	38.563276	69.834241
954.127986	55.964365	69.839246
953.596766	45.994726	69.844250
953.158129	39.728641	69.849255
953.031862	37.834423	69.854260
951.942040	49.310913	69.859265
951.048469	32.862775	69.864270
950.755588	47.989083	69.869274
949.564284	49.506387	69.874279
948.976687	36.005633	69.879284
948.243229	49.487979	69.884289
947.759382	41.306873	69.889294
947.738708	41.939358	69.894298
946.440665	39.007927	69.899303
945.968919	33.510324	69.904308
945.667175	40.457197	69.909313
944.550088	42.047846	69.914318
943.740863	30.722187	69.919322
943.116324	42.955655	69.924327
942.880454	34.134307	69.929332
941.689584	35.099638	69.934337
941.034181	37.884635	69.939342
941.169484	28.949041	69.944346
939.984480	38.348155	69.949351
938.915156	39.314647	69.954356
938.615050	34.534020	69.959361
938.037093	41.717223	69.964366
937.714408	33.461598	69.969370
936.172414	47.506236	69.974375
936.171426	39.320839	69.979380
935.321653	42.551486	69.984385
934.658120	43.491256	69.989390
934.070009	42.607192	69.994394
932.940264	46.221418	69.999399
932.809158	50.452567	70.004404
932.502816	35.987746	70.009409
930.997653	49.920878	70.014414
930.446770	41.463451	70.019418
929.867233	41.825334	70.024423
929.368567	41.371719	70.029428
928.927466	46.989386	70.034433
928.073059	40.012063	70.039438
927.278885	33.832521	70.044442
926.832169	47.969375	70.049447
926.389730	34.004008	70.054452
925.191576	38.193642	70.059457
924.630569	46.963645	70.064462
924.477655	41.621882	70.069466
923.614914	41.752878	70.074471
922.698038	37.425193	70.079476
922.371558	40.534730	70.084481
921.200252	48.578717	70.089486
920.334866	34.215473	70.094490
919.753414	44.341690	70.099495
919.613617	41.372618	70.104500
919.400023	40.253930	70.109505
918.263817	45.810326	70.114510
917.458103	33.730370	70.119514
916.876252	43.243245	70.124519
916.141294	31.457946	70.129524
914.901020	30.412748	70.134529
913.902287	41.475799	70.139534
914.257402	36.127312	70.144538
913.704014	44.541305	70.149543
913.481589	41.992218	70.154548
912.394798	44.410650	70.159553
911.440076	44.415944	70.164558
911.406758	37.033596	70.169562
910.020349	41.264232	70.174567
909.171012	38.523182	70.179572
908.528378	46.290667	70.184577
908.199894	38.898520	70.189582
907.860245	31.128126	70.194586
906.553134	48.692836	70.199591
906.183335	48.311754	70.204596
905.564539	50.868598	70.209601
905.261668	47.919169	70.214606
904.427533	35.779088	70.219610
903.381812	44.028588	70.224615
903.137317	42.823360	70.229620
902.465810	46.200683	70.234625
901.759747	43.876784	70.239630
901.122936	42.874328	70.244634
900.290411	40.687243	70.249639
899.836324	42.033641	70.254644
898.741215	37.456798	70.259649
898.050595	45.118385	70.264654
897.593995	35.460157	70.269658
897.025978	45.141136	70.274663
896.442714	39.631328	70.279668
895.635907	36.817287	70.284673
894.653339	38.424394	70.289678
894.827802	32.473904	70.294682
893.813971	43.164068	70.299687
892.905583	38.634781	70.304692
892.406393	44.121353	70.309697
891.558476	41.865761	70.314702
890.950063	30.027222	70.319706
890.207048	36.840901	70.324711
889.677973	29.565835	70.329716
889.320946	42.020076	70.334721
888.665239	43.795934	70.339726
887.313710	40.001034	70.344730
886.745161	43.141213	70.349735
886.590730	35.221504	70.354740
886.281263	37.390095	70.359745
885.357976	41.925495	70.364750
884.602691	32.789444	70.369754
883.741595	41.930464	70.374759
882.924793	38.316964	70.379764
882.362349	37.176528	70.384769
881.568010	41.536874	70.389774
881.429604	38.991766	70.394778
880.454562	37.998988	70.399783
879.883027	32.119909	70.404788
879.585266	44.985747	70.409793
878.666572	36.452839	70.414798
877.779586	35.471279	70.419802
876.803562	45.888941	70.424807
876.341738	39.314343	70.429812
876.210432	34.666129	70.434817
874.523398	30.522529	70.439822
874.094662	23.231502	70.444826
873.537044	43.242517	70.449831
873.420980	40.206598	70.454836
873.186681	28.575022	70.459841
872.013132	36.953676	70.464846
871.539880	24.253164	70.469850
871.030891	42.234885	70.474855
870.017897	34.634731	70.479860
869.128116	37.974260	70.484865
868.434821	40.035212	70.489870
868.183735	31.621558	70.494874
866.941394	44.254539	70.499879
866.394223	39.833349	70.504884
866.116651	44.384259	70.509889
865.411556	33.472549	70.514894
865.159840	27.255587	70.519898
863.695059	47.205984	70.524903
863.334763	37.545053	70.529908
862.819947	33.525550	70.534913
861.705780	45.928412	70.539918
861.084594	38.827273	70.544922
860.547729	43.528253	70.549927
860.379222	44.632099	70.554932
859.327806	41.029138	70.559937
858.754164	37.242914	70.564942
858.455363	34.463150	70.569946
857.544511	34.027842	70.574951
856.494514	40.657007	70.579956
856.065024	38.301722	70.584961
855.724456	40.770143	70.589966
854.555732	42.066287	70.594970
853.711611	39.359118	70.599975
853.271108	33.946448	70.604980
852.888720	33.102200	70.609985
852.515143	43.606904	70.614990
851.752107	32.912569	70.619994
850.370440	41.997682	70.624999
850.159131	31.407919	70.630004
849.619395	30.645482	70.635009
848.378547	40.037749	70.640014
847.878972	34.006885	70.645018
847.263487	36.888048	70.650023
847.014805	43.414917	70.655028
846.365290	33.650219	70.660033
845.418679	44.298161	70.665038
845.164327	23.610633	70.670042
844.127903	30.813198	70.675047
842.851306	38.878697	70.680052
842.581746	33.831465	70.685057
841.905548	42.301280	70.690062
841.760558	38.680216	70.695066
841.372096	43.382810	70.700071
840.511362	38.806538	70.705076
839.507450	44.960045	70.710081
839.106495	42.671180	70.715086
838.335955	42.226162	70.720090
837.496796	46.972105	70.725095
837.095536	40.215998	70.730100
836.275617	35.579620	70.735105
835.502371	45.433611	70.740110
835.047511	33.463424	70.745114
834.256793	46.339915	70.750119
833.560475	32.260453	70.755124
832.536321	43.231384	70.760129
831.945624	44.470232	70.765134
831.712128	34.204109	70.770138
831.015906	38.520467	70.775143
830.331218	35.245488	70.780148
829.562910	27.790907	70.785153
828.808327	36.590149	70.790158
828.641760	34.814312	70.795162
827.852627	39.172266	70.800167
827.063816	44.283918	70.805172
826.475525	29.565979	70.810177
825.487186	36.975354	70.815182
824.709213	25.685778	70.820186
823.886594	36.367599	70.825191
823.483265	35.275965	70.830196
823.369675	44.608672	70.835201
822.556210	36.492681	70.840206
821.734134	38.963630	70.845210
820.958939	43.253140	70.850215
820.663846	33.747416	70.855220
819.856946	32.994393	70.860225
818.759564	41.487096	70.865230
818.235235	31.150579	70.870234
817.963616	31.769391	70.875239
817.772206	41.727886	70.880244
816.651166	35.472685	70.885249
815.726780	42.390940	70.890254
815.082814	35.558359	70.895258
814.025466	43.946927	70.900263
813.814896	36.031433	70.905268
813.416975	31.729999	70.910273
812.180386	40.110827	70.915278
811.824472	25.256568	70.920282
810.600597	41.554437	70.925287
810.131083	37.101980	70.930292
809.988384	38.704744	70.935297
809.384557	43.936759	70.940302
808.592144	27.508871	70.945306
807.805729	47.677728	70.950311
807.401887	38.794833	70.955316
806.508589	36.975407	70.960321
805.576875	42.756327	70.965326
805.562566	41.184904	70.970330
804.921033	38.147479	70.975335
804.148094	41.634004	70.980340
803.164297	35.000591	70.985345
802.454807	39.891474	70.990350
801.612160	30.507602	70.995354
800.634337	43.243574	71.000359
800.300490	40.677544	71.005364
800.303044	44.417508	71.010369
799.597533	37.129549	71.015374
798.916296	21.461376	71.020378
797.830780	41.859175	71.025383
797.508681	37.550405	71.030388
796.935888	36.581939	71.035393
795.954005	39.472551	71.040398
795.710088	38.921646	71.045402
794.701279	44.355314	71.050407
793.526664	43.033233	71.055412
793.260108	31.116663	71.060417
792.368771	37.578676	71.065422
792.178716	38.130895	71.070426
790.933003	37.176506	71.075431
790.318227	43.078863	71.080436
790.090953	38.310321	71.085441
789.295224	49.300100	71.090446
789.194013	32.511470	71.095450
787.993656	44.343051	71.100455
787.267361	40.254731	71.105460
787.080360	36.192528	71.110465
785.612582	39.736046	71.115470
785.208263	42.787028	71.120474
784.345642	47.785867	71.125479
783.893178	49.731239	71.130484
783.950855	35.369359	71.135489
782.811635	50.915794	71.140494
782.066598	38.238063	71.145498
781.565278	41.395944	71.150503
780.995678	39.395697	71.155508
779.912973	34.766478	71.160513
779.091167	39.689437	71.165518
778.810184	39.801990	71.170522
778.446160	46.012925	71.175527
777.052365	32.640571	71.180532
776.464345	41.298201	71.185537
775.963399	38.984266	71.190542
775.956794	36.853404	71.195546
775.091989	45.250759	71.200551
774.125398	42.490577	71.205556
773.573731	44.221518	71.210561
772.549805	41.956142	71.215566
771.761385	44.494285	71.220570
771.273006	37.975979	71.225575
770.790979	40.350237	71.230580
770.349316	39.575359	71.235585
769.909362	42.384445	71.240590
768.917105	42.778949	71.245594
768.294763	43.018379	71.250599
767.644509	44.824936	71.255604
767.029533	31.445303	71.260609
766.264700	37.787843	71.265614
765.835347	39.363703	71.270618
764.786988	31.012332	71.275623
763.804492	43.824748	71.280628
763.601990	33.679855	71.285633
762.919463	42.459759	71.290638
762.729529	31.784614	71.295642
761.552501	40.712617	71.300647
760.659182	40.619888	71.305652
760.389637	34.568198	71.310657
759.872036	29.196208	71.315662
759.035340	40.820103	71.320666
758.183211	40.047493	71.325671
757.734375	36.627763	71.330676
757.463476	32.637264	71.335681
755.802437	32.081729	71.340686
755.687263	29.088256	71.345690
755.179888	31.696775	71.350695
754.574361	37.405284	71.355700
753.880596	33.665019	71.360705
753.339722	41.380060	71.365710
752.473829	31.900566	71.370714
751.235770	31.011209	71.375719
750.478050	31.647490	71.380724
750.186632	32.854481	71.385729
749.837451	36.435980	71.390734
749.479443	34.883004	71.395738
748.348038	41.493629	71.400743
747.670100	34.798937	71.405748
747.303850	32.168692	71.410753
746.082974	43.569914	71.415758
745.504409	30.700132	71.420762
745.109117	36.297908	71.425767
744.563004	39.664766	71.430772
743.903651	43.092227	71.435777
742.875956	45.644816	71.440782
742.650173	37.506262	71.445786
741.874130	40.066096	71.450791
741.085262	37.386442	71.455796
740.435963	31.775237	71.460801
739.571449	31.438246	71.465806
739.496355	31.901208	71.470810
738.331251	35.406027	71.475815
737.491098	40.130078	71.480820
737.576869	31.298566	71.485825
736.827170	39.641334	71.490830
736.045009	35.479929	71.495834
735.082020	30.156773	71.500839
734.363860	38.854047	71.505844
734.310992	26.621216	71.510849
732.734938	39.625895	71.515854
732.243233	33.428236	71.520858
731.716039	37.821782	71.525863
731.398251	35.860304	71.530868
730.737276	41.842561	71.535873
729.606372	45.464939	71.540878
729.328295	30.227743	71.545882
728.732791	35.731245	71.550887
727.917346	33.954644	71.555892
727.385309	39.541079	71.560897
726.364612	42.786385	71.565902
726.266186	37.897997	71.570906
725.313926	32.464332	71.575911
724.341552	34.074611	71.580916
724.039543	47.712215	71.585921
723.174765	38.063827	71.590926
722.422368	34.575744	71.595930
721.859573	37.450123	71.600935
721.078639	35.264351	71.605940
720.962383	33.955153	71.610945
719.951202	37.660969	71.615950
719.228036	30.623422	71.620954
718.518027	33.265784	71.625959
718.107781	38.198927	71.630964
718.185842	32.396241	71.635969
716.817943	38.722846	71.640974
716.291004	40.352094	71.645978
715.462179	45.392878	71.650983
714.145224	47.360781	71.655988
713.807565	33.624796	71.660993
713.490385	41.909749	71.665998
712.870470	38.859447	71.671002
712.158866	40.268950	71.676007
711.442010	52.108739	71.681012
711.250330	34.325328	71.686017
709.719627	45.640280	71.691022
709.367121	34.678804	71.696026
708.896617	48.302235	71.701031
708.404942	53.295655	71.706036
707.395412	41.071627	71.711041
706.618752	37.472300	71.716046
705.926416	35.642993	71.721050
705.448341	39.784308	71.726055
704.876255	45.739806	71.731060
704.023419	41.624353	71.736065
702.774690	41.540924	71.741070
702.656110	35.141949	71.746074
702.478868	44.845886	71.751079
701.718944	38.135877	71.756084
701.020636	36.758508	71.761089
700.258544	50.616013	71.766094
699.973708	45.714728	71.771098
698.637374	37.800300	71.776103
697.787906	38.511126	71.781108
697.515892	37.627253	71.786113
697.053991	49.379144	71.791118
696.543237	36.471773	71.796122
695.471564	44.529940	71.801127
694.825223	37.240483	71.806132
694.397088	38.551246	71.811137
693.255749	49.812101	71.816142
692.871160	41.889640	71.821146
692.199489	33.527214	71.826151
691.699158	43.093365	71.831156
691.144524	41.196408	71.836161
690.198627	49.934687	71.841166
689.762303	42.706403	71.846170
689.159878	34.291954	71.851175
688.033926	42.040237	71.856180
687.950065	39.795527	71.861185
686.742424	41.823305	71.866190
686.460321	38.992024	71.871194
685.135628	40.779832	71.876199
684.566411	38.818970	71.881204
684.475439	28.850294	71.886209
683.807388	38.501492	71.891214
683.234890	30.419733	71.896218
682.274408	40.374522	71.901223
681.550836	44.127597	71.906228
681.426804	33.686389	71.911233
679.952462	36.586068	71.916238
679.514014	33.858526	71.921242
679.285993	44.076723	71.926247
678.731204	37.559555	71.931252
677.932824	28.887745	71.936257
676.925247	41.188536	71.941262
676.346854	32.216784	71.946266
675.918659	37.406665	71.951271
674.801642	36.718836	71.956276
674.140773	29.393858	71.961281
673.241374	35.693193	71.966286
673.164825	32.250475	71.971290
672.934698	33.342065	71.976295
671.634523	38.882086	71.981300
671.026559	42.684562	71.986305
670.860145	38.508712	71.991310
670.028622	36.960184	71.996314
669.065162	40.470774	72.001319
668.288823	40.420950	72.006324
668.370573	33.919123	72.011329
666.891933	47.248935	72.016334
666.500722	29.744881	72.021338
665.722100	30.710928	72.026343
665.039841	36.132065	72.031348
664.052056	32.154807	72.036353
663.388537	32.626311	72.041358
663.027516	28.590257	72.046362
662.804405	33.875210	72.051367
662.312042	38.931816	72.056372
661.438056	36.443928	72.061377
660.511852	35.391426	72.066382
660.269682	27.632374	72.071386
659.014352	33.236219	72.076391
658.260462	35.023034	72.081396
657.943825	24.183596	72.086401
657.497404	49.677041	72.091406
656.596760	38.301409	72.096410
656.127490	45.396391	72.101415
654.905602	42.314229	72.106420
654.863290	32.638990	72.111425
653.911238	44.924642	72.116430
653.117926	36.196840	72.121434
652.733703	36.529263	72.126439
651.956038	33.701207	72.131444
651.257147	36.065863	72.136449
649.993852	44.000024	72.141454
650.001339	40.256934	72.146458
649.551038	29.744690	72.151463
648.935260	44.304260	72.156468
648.044310	38.056660	72.161473
647.267980	40.644950	72.166478
646.799423	33.145862	72.171482
646.204532	43.204867	72.176487
645.605458	43.574656	72.181492
645.028583	23.878367	72.186497
643.826207	72.766859	72.191502
642.977762	23.131119	72.196506
642.273201	48.954234	72.201511
641.986537	42.079004	72.206516
642.144285	25.212914	72.211521
640.668370	49.643482	72.216526
640.177757	33.676944	72.221530
639.751612	28.536416	72.226535
638.607815	29.425008	72.231540
638.039507	30.084775	72.236545
637.422601	40.268704	72.241550
636.850577	30.537475	72.246554
636.106567	39.737177	72.251559
634.939934	38.284598	72.256564
634.779768	30.876749	72.261569
634.131429	41.857274	72.266574
633.825735	28.087844	72.271578
632.815727	32.241335	72.276583
632.058705	27.899357	72.281588
631.561451	40.536768	72.286593
630.839482	42.275933	72.291598
630.003559	40.373323	72.296602
629.682023	35.827963	72.301607
628.588392	26.181377	72.306612
628.415799	42.545275	72.311617
627.641643	39.544788	72.316622
627.310414	22.570496	72.321626
626.470320	49.213089	72.326631
625.048617	42.310460	72.331636
624.449665	32.777478	72.336641
624.131256	32.143841	72.341646
623.877768	49.033110	72.346650
623.283104	24.380397	72.351655
621.857811	38.996336	72.356660
621.683109	33.911959	72.361665
620.941983	40.100956	72.366670
620.250125	32.053992	72.371674
619.514390	39.949883	72.376679
618.800551	40.563447	72.381684
618.444073	37.223652	72.386689
617.583079	45.071688	72.391694
617.285020	37.051894	72.396698
616.320801	38.585224	72.401703
615.629238	49.853325	72.406708
614.763102	43.330562	72.411713
613.860032	43.464932	72.416718
613.575392	37.316327	72.421722
613.277397	36.610058	72.426727
612.133561	40.365422	72.431732
611.585554	38.790688	72.436737
610.656970	44.331486	72.441742
610.244194	32.638506	72.446746
610.066160	36.323644	72.451751
609.445603	39.905798	72.456756
608.609753	36.863106	72.461761
607.857105	43.359855	72.466766
606.997010	31.457428	72.471770
606.139681	40.027087	72.476775
605.430850	45.488740	72.481780
605.627557	38.561773	72.486785
604.292386	43.875601	72.491790
603.314379	36.858178	72.496794
602.691044	31.137233	72.501799
602.561574	36.446699	72.506804
602.208651	37.647732	72.511809
601.307342	45.104820	72.516814
600.344648	33.409535	72.521818
599.867022	36.204145	72.526823
599.013805	32.448324	72.531828
598.038953	31.804118	72.536833
597.658927	42.040211	72.541838
597.340912	23.649369	72.546842
596.920441	23.678506	72.551847
595.611133	38.009494	72.556852
595.074331	36.814583	72.561857
594.307347	38.031097	72.566862
593.971083	32.513583	72.571866
592.910093	34.249981	72.576871
592.130626	33.446935	72.581876
591.988610	31.897433	72.586881
591.364542	37.227321	72.591886
590.782588	31.750512	72.596890
590.132385	26.153694	72.601895
589.210254	36.933410	72.606900
589.016785	25.839418	72.611905
587.733869	37.272648	72.616910
587.027053	28.736097	72.621914
586.913547	32.065623	72.626919
585.923146	37.859110	72.631924
585.423901	36.513147	72.636929
584.633794	38.340443	72.641934
583.817315	32.065244	72.646938
582.840927	32.682785	72.651943
582.172163	40.478137	72.656948
581.809295	30.946994	72.661953
581.356526	38.083505	72.666958
581.075719	28.696982	72.671962
580.071424	39.585976	72.676967
579.462152	43.532174	72.681972
579.021288	30.178502	72.686977
577.452670	29.736094	72.691982
576.876612	27.743236	72.696986
576.761556	37.131347	72.701991
575.951948	36.539676	72.706996
575.747800	28.099684	72.712001
574.787321	36.745698	72.717006
574.198259	34.754910	72.722010
573.674518	41.013371	72.727015
572.559240	47.610459	72.732020
571.835989	39.450243	72.737025
570.943677	44.674634	72.742030
570.913393	41.468967	72.747034
570.057516	30.933034	72.752039
568.954103	45.477239	72.757044
568.415847	42.951685	72.762049
568.278289	49.473481	72.767054
567.565701	39.980688	72.772058
566.937059	38.857178	72.777063
565.811291	47.876436	72.782068
565.374846	35.289997	72.787073
564.978202	37.571847	72.792078
564.198920	37.967203	72.797082
563.643934	41.102129	72.802087
562.964848	47.429488	72.807092
562.228947	42.494416	72.812097
561.091973	48.837934	72.817102
560.596445	35.839881	72.822106
560.334354	44.989653	72.827111
559.705791	35.172840	72.832116
558.723086	35.770898	72.837121
557.694366	43.256174	72.842126
557.127782	39.360103	72.847130
557.104792	42.359842	72.852135
556.444750	44.525958	72.857140
555.690258	30.848525	72.862145
554.678302	38.845189	72.867150
554.387067	37.953357	72.872154
553.525711	39.577555	72.877159
552.557409	36.906045	72.882164
552.240089	38.577629	72.887169
551.630031	47.603061	72.892174
551.280709	43.552545	72.897178
550.282799	36.478396	72.902183
549.591495	46.633192	72.907188
549.024137	45.195588	72.912193
547.971424	43.556182	72.917198
547.362527	44.692341	72.922202
547.132671	42.004139	72.927207
546.593846	47.866060	72.932212
545.673127	40.942035	72.937217
544.802539	52.941946	72.942222
544.516098	38.658558	72.947226
544.069765	44.858966	72.952231
542.940299	44.986845	72.957236
542.801776	34.529045	72.962241
541.336537	45.660196	72.967246
540.151227	42.958602	72.972250
539.819518	46.764410	72.977255
539.419673	40.457556	72.982260
539.098621	40.439331	72.987265
538.629550	44.156636	72.992270
538.310718	35.848447	72.997274
537.320372	47.031689	73.002279
536.449412	28.877157	73.007284
535.636794	29.520669	73.012289
534.662910	35.503919	73.017294
534.173114	38.612698	73.022298
533.855537	37.043856	73.027303
533.290856	45.202667	73.032308
532.740158	38.339555	73.037313
531.852609	34.278584	73.042318
531.143087	40.148771	73.047322
530.339031	34.029300	73.052327
529.222668	44.048384	73.057332
529.201493	31.983988	73.062337
528.528428	45.467808	73.067342
527.833612	42.634481	73.072346
526.959347	44.366395	73.077351
526.184493	45.779716	73.082356
526.087687	33.739980	73.087361
525.591587	42.751992	73.092366
524.109924	43.327041	73.097370
524.115947	41.796538	73.102375
523.021047	44.013005	73.107380
522.791683	34.482686	73.112385
521.575392	38.320588	73.117390
521.175092	37.714200	73.122394
520.753513	34.859431	73.127399
519.819571	37.152756	73.132404
519.046378	37.345316	73.137409
518.422933	42.244636	73.142414
517.750960	27.054476	73.147418
517.509901	47.578016	73.152423
516.547704	34.821460	73.157428
516.284005	34.216967	73.162433
515.676135	38.941927	73.167438
514.486471	32.098603	73.172442
513.742075	50.297594	73.177447
513.056297	44.972951	73.182452
512.850411	34.388699	73.187457
511.651480	40.392037	73.192462
511.087618	43.755457	73.197466
510.511879	30.628284	73.202471
510.141752	29.933518	73.207476
509.317086	36.757133	73.212481
508.220363	48.077169	73.217486
507.717468	30.532617	73.222490
507.610204	29.431724	73.227495
506.544864	53.579334	73.232500
505.593321	34.655519	73.237505
504.963298	38.530923	73.242510
504.861241	35.702527	73.247514
504.650690	37.133194	73.252519
503.490068	40.632671	73.257524
503.043405	37.684134	73.262529
502.290660	34.139415	73.267534
501.102533	26.379696	73.272538
500.705437	49.342277	73.277543
500.217573	34.931724	73.282548
499.881063	28.917556	73.287553
498.613622	53.914178	73.292558
497.974793	28.073290	73.297562
497.454536	40.588223	73.302567
496.684586	49.612327	73.307572
496.182684	30.629514	73.312577
495.293672	40.240250	73.317582
494.892392	47.396956	73.322586
494.176709	33.339649	73.327591
493.021988	34.192202	73.332596
492.929974	37.100437	73.337601
492.267926	50.177255	73.342606
491.407527	41.105408	73.347610
490.724768	31.382407	73.352615
489.799404	43.167132	73.357620
489.578380	32.175311	73.362625
488.984796	40.072239	73.367630
488.280365	36.109841	73.372634
487.457303	39.475132	73.377639
486.856014	36.890258	73.382644
486.346638	32.985095	73.387649
485.481900	39.167007	73.392654
484.786896	39.422812	73.397658
484.420921	32.544484	73.402663
483.220407	38.869766	73.407668
482.695514	40.022519	73.412673
481.949666	37.287218	73.417678
481.461622	35.570507	73.422682
481.336450	38.236455	73.427687
480.174305	36.961423	73.432692
479.921407	41.038517	73.437697
479.164486	36.630345	73.442702
478.035495	36.873289	73.447706
477.313110	31.877753	73.452711
476.659578	42.020233	73.457716
476.299621	39.603487	73.462721
476.128586	35.415782	73.467726
474.791370	38.397806	73.472730
474.233711	32.598633	73.477735
473.660446	29.514163	73.482740
473.019881	26.192846	73.487745
472.285169	33.759035	73.492750
471.468116	35.557542	73.497754
471.092375	34.912560	73.502759
470.007782	43.106895	73.507764
469.351755	33.685555	73.512769
469.111148	32.714710	73.517774
468.796440	28.267636	73.522778
468.230097	28.275880	73.527783
466.776381	35.499320	73.532788
466.078295	33.183748	73.537793
465.727182	39.577141	73.542798
465.217348	37.718832	73.547802
464.567836	27.082270	73.552807
463.467220	37.469428	73.557812
463.178075	23.862984	73.562817
462.030416	31.662107	73.567822
461.283483	30.748271	73.572826
461.006398	34.584803	73.577831
460.509756	33.698899	73.582836
460.063645	33.828333	73.587841
459.260710	32.819345	73.592846
458.650127	28.504559	73.597850
458.576783	17.935482	73.602855
457.043383	41.389711	73.607860
456.528259	35.284161	73.612865
456.051272	34.194864	73.617870
454.623682	34.047018	73.622874
454.387617	26.236574	73.627879
453.566736	26.614937	73.632884
453.007529	31.915595	73.637889
452.748235	33.447065	73.642894
451.820565	25.729455	73.647898
451.315264	31.860419	73.652903
450.553119	17.148264	73.657908
449.901543	25.754557	73.662913
448.877815	24.481143	73.667918
448.229740	21.638822	73.672922
447.949760	26.209057	73.677927
447.446028	26.290906	73.682932
446.617399	22.468154	73.687937
445.868379	21.152554	73.692942
445.465648	20.882440	73.697946
444.563475	17.700577	73.702951
443.426235	25.963220	73.707956
443.308081	25.436469	73.712961
442.802154	28.871089	73.717966
441.701829	29.238785	73.722970
441.069194	21.523062	73.727975
440.430938	21.098093	73.732980
440.135441	20.888163	73.737985
439.729962	23.575113	73.742990
438.503384	19.525621	73.747994
437.916315	24.048591	73.752999
437.525115	37.120098	73.758004
436.706753	19.066058	73.763009
435.924763	29.626372	73.768014
434.919869	19.677193	73.773018
434.846722	18.679673	73.778023
433.774593	28.131943	73.783028
433.233210	13.939686	73.788033
432.559469	20.556352	73.793038
432.057821	27.416824	73.798042
431.962804	25.088758	73.803047
430.737234	34.392024	73.808052
429.957897	26.212422	73.813057
429.539815	24.653302	73.818062
428.393958	27.699471	73.823066
427.799973	26.764432	73.828071
427.355920	31.327696	73.833076
426.836967	26.276115	73.838081
426.402082	23.109691	73.843086
425.233707	24.615697	73.848090
424.825083	17.365735	73.853095
424.316014	34.283075	73.858100
423.045975	33.518820	73.863105
422.254233	25.738569	73.868110
421.455856	31.712814	73.873114
421.501194	34.618088	73.878119
420.748191	32.166207	73.883124
420.564201	23.097017	73.888129
419.763637	29.937311	73.893134
419.044624	28.932312	73.898138
418.192430	22.923056	73.903143
417.013025	35.096755	73.908148
416.673660	36.193156	73.913153
416.435487	35.373307	73.918158
415.651479	28.244649	73.923162
415.360287	22.825643	73.928167
414.240603	35.637920	73.933172
413.917201	28.558871	73.938177
412.555880	28.392607	73.943182
411.835555	28.203060	73.948186
411.324152	24.113748	73.953191
410.844541	37.093691	73.958196
410.528681	25.986122	73.963201
409.676045	28.116728	73.968206
408.803777	36.613125	73.973210
408.460053	27.113669	73.978215
407.402468	29.620688	73.983220
407.019766	25.028349	73.988225
406.369779	32.778162	73.993230
405.590788	27.985626	73.998234
404.867499	29.882748	74.003239
403.903216	33.839813	74.008244
403.756161	29.154738	74.013249
403.301398	25.450619	74.018254
402.150404	31.700237	74.023258
401.406642	21.567550	74.028263
400.638642	27.243662	74.033268
400.332193	27.760839	74.038273
399.826680	22.199375	74.043278
398.632446	18.933184	74.048282
398.439113	16.683862	74.053287
397.772342	24.081550	74.058292
397.097869	17.309169	74.063297
396.336624	23.864096	74.068302
395.606159	33.019106	74.073306
395.358305	24.770605	74.078311
393.884507	31.628293	74.083316
393.530448	13.232237	74.088321
393.016816	36.011516	74.093326
392.606548	30.173115	74.098330
392.364600	11.756045	74.103335
391.099168	21.704300	74.108340
390.473473	32.148263	74.113345
389.330936	31.906153	74.118350
388.158409	26.660692	74.123354
388.117273	19.043119	74.128359
387.248152	32.830981	74.133364
387.269191	18.386705	74.138369
386.809339	29.862319	74.143374
385.983758	31.841974	74.148378
385.421473	22.546077	74.153383
384.533604	32.770055	74.158388
384.253226	34.453117	74.163393
382.963128	36.358563	74.168398
382.369460	37.713095	74.173402
382.025390	21.459982	74.178407
381.149765	31.626819	74.183412
380.479210	35.045107	74.188417
379.877564	21.431714	74.193422
379.378137	30.149389	74.198426
378.725525	21.161185	74.203431
377.432265	40.243949	74.208436
376.800714	19.049014	74.213441
376.726378	27.285814	74.218446
376.239865	25.067439	74.223450
375.484621	20.250634	74.228455
374.715741	31.176281	74.233460
373.793492	19.767978	74.238465
372.790698	27.044184	74.243470
372.174633	32.871127	74.248474
371.985932	26.122266	74.253479
371.423297	33.445028	74.258484
370.596331	29.054365	74.263489
370.108631	34.821435	74.268494
369.285015	25.366920	74.273498
369.138080	7.024605	74.278503
367.684581	22.941310	74.283508
366.978032	25.627361	74.288513
366.681978	30.200164	74.293518
365.956429	37.074250	74.298522
365.081288	25.748322	74.303527
364.534322	21.677304	74.308532
364.236407	26.617812	74.313537
363.733342	39.705571	74.318542
362.478698	32.489507	74.323546
362.222387	32.230766	74.328551
361.170808	31.116360	74.333556
360.564533	35.725983	74.338561
359.842628	30.976403	74.343566
359.072955	38.319544	74.348570
358.684506	38.957021	74.353575
358.157889	44.697182	74.358580
357.060003	42.432735	74.363585
356.628750	34.110964	74.368590
355.820291	27.657971	74.373594
355.786062	20.665315	74.378599
354.794199	28.810215	74.383604
353.869362	26.456699	74.388609
353.469240	32.498380	74.393614
353.189445	32.167693	74.398618
352.381194	34.043677	74.403623
350.985995	34.491516	74.408628
350.795995	26.068233	74.413633
350.364597	15.535732	74.418638
348.760622	29.691419	74.423642
348.526348	23.148510	74.428647
347.766706	35.077157	74.433652
347.463297	32.403855	74.438657
347.497284	34.014749	74.443662
346.450390	44.434388	74.448666
345.641946	25.749637	74.453671
345.070836	35.008568	74.458676
344.002312	20.408357	74.463681
343.298681	26.246104	74.468686
342.300605	35.333391	74.473690
342.319210	28.261355	74.478695
341.580541	40.451578	74.483700
341.111409	26.858077	74.488705
340.299320	29.740717	74.493710
339.718087	33.457000	74.498714
338.888003	20.561234	74.503719
337.770403	32.417620	74.508724
337.568223	33.865886	74.513729
336.860830	35.613846	74.518734
335.970433	34.166276	74.523738
335.771213	26.214371	74.528743
334.542565	36.601473	74.533748
334.494856	29.131597	74.538753
333.854225	31.852882	74.543758
332.830068	35.048425	74.548762
332.513126	25.869556	74.553767
331.959411	37.148837	74.558772
331.122109	35.263900	74.563777
330.181995	32.934903	74.568782
329.579627	34.298718	74.573786
329.325500	33.287467	74.578791
327.878852	40.710115	74.583796
327.589929	38.300997	74.588801
327.045171	39.731322	74.593806
326.376393	39.640812	74.598810
325.899257	34.566823	74.603815
325.009426	38.524666	74.608820
324.500997	35.360520	74.613825
323.951049	43.442898	74.618830
322.667820	41.980668	74.623834
322.254995	37.891433	74.628839
321.638581	35.990221	74.633844
321.169067	39.075304	74.638849
320.131188	37.380022	74.643854
319.570175	35.195607	74.648858
319.143157	32.944109	74.653863
318.473281	38.268735	74.658868
317.765056	38.971371	74.663873
317.265576	29.670213	74.668878
316.520796	41.489275	74.673882
316.042672	25.667527	74.678887
314.572154	35.038259	74.683892
314.046554	27.203022	74.688897
313.729581	32.898738	74.693902
313.397132	31.297608	74.698906
312.766879	31.978357	74.703911
311.778964	38.317135	74.708916
311.469643	36.117840	74.713921
310.579160	36.289735	74.718926
309.557381	31.234744	74.723930
309.500546	24.076970	74.728935
308.493727	33.266578	74.733940
307.770993	30.205972	74.738945
307.106311	32.667761	74.743950
306.174963	32.075083	74.748954
305.809421	28.987513	74.753959
305.216416	40.930614	74.758964
304.341878	30.536543	74.763969
303.925299	33.450774	74.768974
303.080648	40.509428	74.773978
303.089518	39.572953	74.778983
301.540341	40.436423	74.783988
300.959556	36.351885	74.788993
300.869405	32.946051	74.793998
300.149548	40.347496	74.799002
299.137440	40.439436	74.804007
298.486138	33.762732	74.809012
298.077796	27.914586	74.814017
297.544983	32.337480	74.819022
296.365753	43.404239	74.824026
295.718426	34.413638	74.829031
294.998493	37.052960	74.834036
294.916312	35.104457	74.839041
294.058126	29.553496	74.844046
293.009874	45.128142	74.849050
292.770219	29.673647	74.854055
292.054655	42.935621	74.859060
291.228646	31.701235	74.864065
290.533925	25.692164	74.869070
290.078953	37.654263	74.874074
289.839263	22.262857	74.879079
288.805508	36.827568	74.884084
287.860811	50.509246	74.889089
287.529536	33.699053	74.894094
286.547678	37.294704	74.899098
286.258808	38.630641	74.904103
285.155276	28.612103	74.909108
284.948497	29.772539	74.914113
283.893623	27.206400	74.919118
283.017982	27.306558	74.924122
282.541388	26.570452	74.929127
282.125166	37.655946	74.934132
281.638395	36.358522	74.939137
280.442126	31.646728	74.944142
280.373825	23.437438	74.949146
279.821109	47.057119	74.954151
278.814766	32.503792	74.959156
277.830868	31.910039	74.964161
277.522489	28.404956	74.969166
276.836715	36.001233	74.974170
276.373689	28.266415	74.979175
275.546873	27.012151	74.984180
275.028361	32.036708	74.989185
274.294488	26.458059	74.994190
273.077971	32.853782	74.999194
272.754312	25.465739	75.004199
272.013333	36.822178	75.009204
271.728159	33.835339	75.014209
270.830006	37.428693	75.019214
269.709997	42.735193	75.024218
269.752586	28.822049	75.029223
269.139073	27.816048	75.034228
268.396014	34.976781	75.039233
267.667587	26.120540	75.044238
266.929945	33.691971	75.049242
266.370607	21.935735	75.054247
265.531269	24.996194	75.059252
264.904701	31.506037	75.064257
264.521312	26.123827	75.069262
263.407297	32.266687	75.074266
262.845094	21.185807	75.079271
261.791990	22.353411	75.084276
261.632662	24.212720	75.089281
261.509198	30.749601	75.094286
260.147711	28.292264	75.099290
259.938379	33.381079	75.104295
258.842571	32.895052	75.109300
257.891521	33.164925	75.114305
257.019594	27.900005	75.119310
256.804451	35.653072	75.124314
256.467467	28.844288	75.129319
256.069491	16.095723	75.134324
255.117814	29.639737	75.139329
254.554417	26.569522	75.144334
253.553950	34.143426	75.149338
253.134957	23.746157	75.154343
251.967105	35.383514	75.159348
251.428672	22.785058	75.164353
251.084778	17.861735	75.169358
250.591002	32.269424	75.174362
250.020869	29.599230	75.179367
248.785398	39.235290	75.184372
248.190395	27.543084	75.189377
247.909378	22.026298	75.194382
246.666174	34.801548	75.199386
246.022334	30.736539	75.204391
245.750719	23.273980	75.209396
245.533332	31.995597	75.214401
244.951588	34.657057	75.219406
243.870397	39.258829	75.224410
243.467698	28.808502	75.229415
242.160506	36.566911	75.234420
241.203196	21.917497	75.239425
241.040585	26.331850	75.244430
240.414583	30.928870	75.249434
240.338975	23.991702	75.254439
238.850997	35.274837	75.259444
238.355804	29.771689	75.264449
238.074080	21.668959	75.269454
237.325742	27.258404	75.274458
236.505799	24.566535	75.279463
235.864423	38.969376	75.284468
235.287514	20.848571	75.289473
234.830963	28.111864	75.294478
233.521373	35.946349	75.299482
232.911468	26.041537	75.304487
232.467663	27.526747	75.309492
231.834716	30.417132	75.314497
231.429921	19.511436	75.319502
230.452641	32.780436	75.324506
230.277944	17.421267	75.329511
229.362571	31.552403	75.334516
228.407933	17.913343	75.339521
227.742479	30.752612	75.344526
227.268734	32.149562	75.349530
226.677887	19.226754	75.354535
225.597894	25.927142	75.359540
225.106289	34.728739	75.364545
225.032156	20.654452	75.369550
224.231392	34.497679	75.374554
223.239175	27.460630	75.379559
222.144430	30.743156	75.384564
222.110069	24.012292	75.389569
221.494576	20.198227	75.394574
220.426055	28.017939	75.399578
219.943304	23.433704	75.404583
219.424336	22.103581	75.409588
218.908589	22.043897	75.414593
217.796975	28.817135	75.419598
217.080276	24.743251	75.424602
216.992222	21.934724	75.429607
216.252680	22.979827	75.434612
215.161728	27.978955	75.439617
214.499709	20.964968	75.444622
214.261663	27.881213	75.449626
213.543735	19.553151	75.454631
212.565832	25.362111	75.459636
211.785403	31.860221	75.464641
211.506556	29.320213	75.469646
210.804818	25.980342	75.474650
210.320507	28.728773	75.479655
209.421606	27.943313	75.484660
209.041082	27.070490	75.489665
208.447693	32.873350	75.494670
207.273236	31.762831	75.499674
207.107854	30.606568	75.504679
206.035508	33.336781	75.509684
205.123544	35.182038	75.514689
204.699057	35.804783	75.519694
203.785462	31.532067	75.524698
203.900836	33.894762	75.529703
202.846642	27.596114	75.534708
202.090711	35.159437	75.539713
201.484115	26.610211	75.544718
201.050943	25.663785	75.549722
199.922433	30.000317	75.554727
199.156056	31.295695	75.559732
198.702963	37.194458	75.564737
198.447302	41.347698	75.569742
197.829209	37.955073	75.574746
197.074190	29.434238	75.579751
196.373296	31.077126	75.584756
195.404666	37.775547	75.589761
194.572941	36.129453	75.594766
193.603289	30.878561	75.599770
193.472372	25.452966	75.604775
193.140019	32.769003	75.609780
192.537417	30.518715	75.614785
191.752315	31.987381	75.619790
190.819721	43.122087	75.624794
190.860302	22.390917	75.629799
189.609843	32.224916	75.634804
188.886926	31.660554	75.639809
188.400304	35.576238	75.644814
187.638801	32.045638	75.649818
186.821202	21.358717	75.654823
185.973732	32.590226	75.659828
185.463491	32.986962	75.664833
185.331047	31.115861	75.669838
184.235278	36.429567	75.674842
183.727985	32.369616	75.679847
183.135132	32.617104	75.684852
182.536162	38.450821	75.689857
181.670645	32.833269	75.694862
180.843203	34.658752	75.699866
180.364050	27.301825	75.704871
179.949189	28.205298	75.709876
178.959376	30.321580	75.714881
178.190761	27.821811	75.719886
177.436677	31.571988	75.724890
177.309790	27.437203	75.729895
176.258955	37.261463	75.734900
175.400895	32.696070	75.739905
175.177517	34.693321	75.744910
175.028563	36.965697	75.749914
173.953141	25.094658	75.754919
173.008666	27.389784	75.759924
172.355405	32.003779	75.764929
171.976423	31.414551	75.769934
170.521463	33.154009	75.774938
170.297524	28.642058	75.779943
169.675951	34.409997	75.784948
169.122157	33.317235	75.789953
168.678444	21.474796	75.794958
167.647788	27.858276	75.799962
167.107377	27.387819	75.804967
166.587056	33.339878	75.809972
166.217721	21.846683	75.814977
165.550704	25.239226	75.819982
164.635572	27.395643	75.824986
163.998864	26.648820	75.829991
162.831872	34.487408	75.834996
162.159839	36.906252	75.840001
162.136570	23.224388	75.845006
161.324814	26.039223	75.850010
160.466488	34.311122	75.855015
159.830875	34.393555	75.860020
159.471238	26.662786	75.865025
158.624394	28.611211	75.870030
157.457414	32.819860	75.875034
157.088965	26.165918	75.880039
156.773622	32.414862	75.885044
156.133009	26.586435	75.890049
155.213821	33.759504	75.895054
154.332443	37.706592	75.900058
153.903731	31.465932	75.905063
153.454900	29.913342	75.910068
152.856786	29.740655	75.915073
152.113293	27.490764	75.920078
151.063186	32.830316	75.925082
150.545748	19.768108	75.930087
149.572512	27.813913	75.935092
148.890854	27.720774	75.940097
148.966070	15.920184	75.945102
148.303424	23.878624	75.950106
147.421939	24.373977	75.955111
146.237863	30.067607	75.960116
146.051305	23.031452	75.965121
145.934042	12.959832	75.970126
144.570877	32.058534	75.975130
143.829955	19.842466	75.980135
143.480515	24.982003	75.985140
142.969112	29.847761	75.990145
141.731792	24.146013	75.995150
140.622170	36.258222	76.000154
140.537409	16.256644	76.005159
140.051711	27.640202	76.010164
139.916760	19.810544	76.015169
139.330007	30.768695	76.020174
138.610833	28.639504	76.025178
137.627073	24.512038	76.030183
136.455608	32.113242	76.035188
136.145054	27.496841	76.040193
135.570363	23.889171	76.045198
134.211891	37.266281	76.050202
133.550719	39.418488	76.055207
133.250271	36.697440	76.060212
132.830818	23.903447	76.065217
132.765255	28.866846	76.070222
131.482788	32.759625	76.075226
130.787662	29.879169	76.080231
130.035134	29.226511	76.085236
129.751628	27.868327	76.090241
129.094895	23.327622	76.095246
128.269013	28.204101	76.100250
127.773883	28.153764	76.105255
126.817231	30.979097	76.110260
125.997249	30.622607	76.115265
125.559931	24.052189	76.120270
124.968038	29.384919	76.125274
124.456711	26.874106	76.130279
123.484863	33.107886	76.135284
123.020405	28.370955	76.140289
122.739405	25.695693	76.145294
121.283432	34.709406	76.150298
120.712970	22.336865	76.155303
120.591412	37.232388	76.160308
119.554656	28.865310	76.165313
118.793808	17.581205	76.170318
118.043856	30.325157	76.175322
117.234912	23.151713	76.180327
117.024323	29.256230	76.185332
116.640410	36.381809	76.190337
115.663557	24.496665	76.195342
114.966156	33.786799	76.200346
114.522635	34.215486	76.205351
113.007655	35.751671	76.210356
112.982707	33.227959	76.215361
112.565585	42.793513	76.220366
111.950104	36.057546	76.225370
111.288380	30.618829	76.230375
110.264045	30.562995	76.235380
109.849566	37.363884	76.240385
108.946674	32.614866	76.245390
108.021622	31.978685	76.250394
107.695782	30.977318	76.255399
107.305814	31.353315	76.260404
106.488345	37.198231	76.265409
105.704493	28.956406	76.270414
104.900451	29.209204	76.275418
104.779215	20.305097	76.280423
103.522252	36.318314	76.285428
102.384546	32.524473	76.290433
102.396591	27.985942	76.295438
101.687263	40.717121	76.300442
101.622520	24.813771	76.305447
100.780702	27.081515	76.310452
99.827261	30.250102	76.315457
99.375660	35.631428	76.320462
98.214931	25.026064	76.325466
97.453928	28.901938	76.330471
97.206635	21.900704	76.335476
96.353961	29.608777	76.340481
95.798914	24.745957	76.345486
94.548927	35.231165	76.350490
94.240150	26.845787	76.355495
94.003705	27.976276	76.360500
93.427910	31.234450	76.365505
93.071235	25.436457	76.370510
92.066856	38.334524	76.375514
91.342288	20.213676	76.380519
90.206292	32.408946	76.385524
89.107754	25.926627	76.390529
89.138556	21.208499	76.395534
88.323915	31.534406	76.400538
88.239103	22.720681	76.405543
87.357483	33.855162	76.410548
86.260370	32.617258	76.415553
86.313252	20.228909	76.420558
85.622066	35.070186	76.425562
84.781471	27.045564	76.430567
83.790120	8.022735	76.435572
83.111229	17.762472	76.440577
82.739213	26.655390	76.445582
81.523503	30.822959	76.450586
81.313821	23.360017	76.455591
80.670651	28.108032	76.460596
80.438962	39.257146	76.465601
79.406988	27.812868	76.470606
78.455348	26.034561	76.475610
77.976138	29.159071	76.480615
77.478469	27.104958	76.485620
76.504831	29.210815	76.490625
75.882731	22.941095	76.495630
75.220955	30.137790	76.500634
75.000127	29.756734	76.505639
73.860635	25.362411	76.510644
73.239820	31.898177	76.515649
72.793717	33.998757	76.520654
71.847536	32.615374	76.525658
71.296082	29.833444	76.530663
70.458099	29.039899	76.535668
70.074997	32.686795	76.540673
69.911915	28.307071	76.545678
68.608860	42.227277	76.550682
67.813855	31.588836	76.555687
67.322467	34.808325	76.560692
67.089491	34.438668	76.565697
66.060896	35.222422	76.570702
65.295355	33.980536	76.575706
64.571470	40.833925	76.580711
64.458238	38.276987	76.585716
63.442630	28.008025	76.590721
62.984368	27.712138	76.595726
62.231024	35.024359	76.600730
61.443752	33.596716	76.605735
60.360312	31.615519	76.610740
60.067703	27.092459	76.615745
59.678026	32.153272	76.620750
59.065906	32.980994	76.625754
58.067152	32.839106	76.630759
57.346962	35.382343	76.635764
56.860364	30.175899	76.640769
56.579282	20.475745	76.645774
55.155131	31.487028	76.650778
54.391058	15.843445	76.655783
53.790302	19.130834	76.660788
53.746133	24.880825	76.665793
53.363174	27.155829	76.670798
52.187876	34.336657	76.675802
51.538687	32.462822	76.680807
51.085798	32.681715	76.685812
50.220862	20.140133	76.690817
49.501474	25.215680	76.695822
48.747922	30.506399	76.700826
48.515778	35.062726	76.705831
47.655544	27.698803	76.710836
46.440638	31.140904	76.715841
46.014353	26.673855	76.720846
45.388538	29.936861	76.725850
45.190370	23.531740	76.730855
44.517719	35.164309	76.735860
43.284240	25.057830	76.740865
43.377237	20.602583	76.745870
42.291752	32.993229	76.750874
41.693942	24.537271	76.755879
41.046404	21.467916	76.760884
40.606758	26.224480	76.765889
39.913361	15.319138	76.770894
39.097892	24.907214	76.775898
38.652916	32.840427	76.780903
37.868047	26.760670	76.785908
36.534135	36.365206	76.790913
36.290622	22.587608	76.795918
35.680530	29.099594	76.800922
35.132908	33.017145	76.805927
34.120651	35.201713	76.810932
33.756530	33.569409	76.815937
33.205406	21.939672	76.820942
32.669776	33.477854	76.825946
31.744740	28.726094	76.830951
30.642335	32.533438	76.835956
30.480814	30.774212	76.840961
30.189894	20.113748	76.845966
28.804151	35.958304	76.850970
28.076001	31.167260	76.855975
27.603609	37.740865	76.860980
27.481932	24.710191	76.865985
26.965072	26.252815	76.870990
25.648705	33.987553	76.875994
25.309819	28.519455	76.880999
24.616195	40.174298	76.886004
23.540683	25.416126	76.891009
22.913724	30.574706	76.896014
22.291053	35.377809	76.901018
22.037266	27.390508	76.906023
21.252208	27.884719	76.911028
20.597899	24.184129	76.916033
20.176630	30.653389	76.921038
19.247441	29.874409	76.926042
18.357215	31.430852	76.931047
17.913977	29.473721	76.936052
17.318640	33.395732	76.941057
16.978633	21.068473	76.946062
15.406420	32.494450	76.951066
15.015569	34.625648	76.956071
15.012941	30.220340	76.961076
13.811177	32.616479	76.966081
13.167519	23.879277	76.971086
12.294233	37.872874	76.976090
11.938385	28.706590	76.981095
11.708662	22.331737	76.986100
10.561787	28.735385	76.991105
10.063929	24.904196	76.996110
9.419559	25.863223	77.001114
8.468866	34.466841	77.006119
7.595522	36.324931	77.011124
7.047311	29.042140	77.016129
7.022592	16.387075	77.021134
6.344969	29.712408	77.026139
5.321094	27.751698	77.031143
4.717594	35.538321	77.036148
4.001547	24.885743	77.041153
3.026614	19.966925	77.046158