Mon Mar 08 18:58:03 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.705333	92.968876	0.000000
0.228005	84.985658	0.005005
-0.725662	41.804053	0.010010
-2.568436	1.229021	0.015014
-7.282140	9.666482	0.020019
-12.216925	14.771058	0.025024
-16.665623	11.052867	0.030029
-21.238247	13.797483	0.035034
-25.184269	10.604636	0.040038
-28.980280	7.208106	0.045043
-33.210052	3.801934	0.050048
-36.293342	7.507407	0.055053
-40.218268	23.324938	0.060058
-43.614756	16.179584	0.065062
-47.373767	18.854378	0.070067
-50.876275	21.792592	0.075072
-54.757728	15.326979	0.080077
-59.013323	16.758029	0.085082
-62.740346	13.331624	0.090086
-66.169021	16.609718	0.095091
-69.937531	8.918245	0.100096
-73.442191	7.455834	0.105101
-77.621319	19.013889	0.110106
-81.104074	11.648981	0.115110
-85.164333	8.982207	0.120115
-89.127995	14.617932	0.125120
-92.669972	11.638261	0.130125
-96.529648	20.657106	0.135130
-100.303855	9.450206	0.140134
-103.996715	12.447247	0.145139
-108.011304	29.925423	0.150144
-111.536364	13.128257	0.155149
-115.554893	20.994567	0.160154
-118.706079	16.546027	0.165158
-122.497382	15.064771	0.170163
-126.059859	4.084317	0.175168
-130.058254	9.088598	0.180173
-134.481127	14.031315	0.185178
-138.181510	-4.410852	0.190182
-142.186550	18.581664	0.195187
-145.897658	20.400617	0.200192
-149.257957	17.764177	0.205197
-153.049143	19.911290	0.210202
-156.410276	7.791802	0.215206
-160.676308	15.387034	0.220211
-164.259404	20.090152	0.225216
-167.920460	13.192193	0.230221
-171.722381	29.983709	0.235226
-175.483666	16.002758	0.240230
-179.043001	11.051767	0.245235
-182.923947	20.665455	0.250240
-186.803306	15.801812	0.255245
-190.701318	18.552620	0.260250
-194.337399	8.023959	0.265254
-197.942589	13.318815	0.270259
-201.826505	8.694031	0.275264
-205.470992	8.928745	0.280269
-209.363916	13.397538	0.285274
-213.291304	10.247759	0.290278
-216.865849	20.124815	0.295283
-220.570441	17.770491	0.300288
-224.430308	10.806588	0.305293
-228.266523	20.840532	0.310298
-231.579474	6.043859	0.315302
-235.584883	5.801670	0.320307
-239.645190	16.678741	0.325312
-243.088758	14.109339	0.330317
-247.056507	18.569636	0.335322
-250.722485	12.897808	0.340326
-254.563263	10.215215	0.345331
-258.168772	6.298247	0.350336
-262.085147	20.548918	0.355341
-265.994313	25.280576	0.360346
-269.232194	8.396839	0.365350
-273.301169	16.873805	0.370355
-277.068071	13.454103	0.375360
-280.637390	15.641688	0.380365
-284.732430	17.640400	0.385370
-288.358323	6.719208	0.390374
-292.183996	19.574125	0.395379
-295.852566	5.091345	0.400384
-299.317163	1.169294	0.405389
-303.788334	21.981557	0.410394
-307.478707	11.663581	0.415398
-311.100242	11.022793	0.420403
-314.684078	24.398922	0.425408
-318.167831	18.452121	0.430413
-322.036628	15.998021	0.435418
-325.686041	9.270335	0.440422
-329.547077	12.531089	0.445427
-333.586459	19.439193	0.450432
-337.249724	7.279912	0.455437
-341.206153	8.775651	0.460442
-345.124680	19.100434	0.465446
-348.621136	14.078166	0.470451
-352.473636	25.024739	0.475456
-355.882113	4.453317	0.480461
-360.008187	15.512953	0.485466
-363.209064	9.778088	0.490470
-367.106645	8.955968	0.495475
-371.234032	17.658444	0.500480
-374.789970	16.991510	0.505485
-379.136493	25.385238	0.510490
-382.704318	28.381659	0.515494
-386.127719	16.967848	0.520499
-390.030397	10.246010	0.525504
-393.837996	2.744231	0.530509
-397.694748	16.075737	0.535514
-401.097436	0.792223	0.540518
-404.763380	26.195588	0.545523
-408.551803	15.984890	0.550528
-412.317954	14.999940	0.555533
-416.200880	11.357732	0.560538
-420.024308	21.683213	0.565542
-423.672448	13.591504	0.570547
-427.695683	9.083955	0.575552
-431.161200	15.624629	0.580557
-435.092612	12.955225	0.585562
-438.923356	5.876657	0.590566
-442.649034	14.612865	0.595571
-446.515764	7.388678	0.600576
-449.598906	7.482084	0.605581
-454.153563	18.457360	0.610586
-457.450550	10.333282	0.615590
-461.376618	6.904607	0.620595
-465.206004	22.190291	0.625600
-468.913590	20.563762	0.630605
-473.024557	25.249131	0.635610
-476.642208	9.927523	0.640614
-480.273612	11.932939	0.645619
-484.296202	9.152033	0.650624
-487.619607	12.907453	0.655629
-491.473754	14.349259	0.660634
-495.314083	15.806209	0.665638
-499.026349	17.709459	0.670643
-502.787828	16.132590	0.675648
-506.505633	16.983402	0.680653
-510.193005	23.207986	0.685658
-514.221365	8.606431	0.690662
-517.923966	12.584872	0.695667
-521.561277	15.546864	0.700672
-525.400534	14.310437	0.705677
-529.166045	21.246072	0.710682
-532.804293	17.563398	0.715686
-536.638375	19.995485	0.720691
-540.252063	19.738541	0.725696
-544.215509	18.171922	0.730701
-548.244144	21.503946	0.735706
-551.778523	10.298925	0.740710
-555.612006	18.797071	0.745715
-559.520027	20.703301	0.750720
-562.594762	18.308823	0.755725
-566.590741	18.235981	0.760730
-570.237552	10.830226	0.765734
-574.364829	19.531441	0.770739
-577.775363	18.412681	0.775744
-581.604711	18.168175	0.780749
-585.981482	20.769030	0.785754
-589.329606	6.159868	0.790758
-593.174763	7.196729	0.795763
-596.956618	22.396166	0.800768
-600.752869	11.955253	0.805773
-604.253652	14.338931	0.810778
-607.825408	20.617722	0.815782
-611.863187	22.544767	0.820787
-615.704223	19.591586	0.825792
-619.233678	11.101214	0.830797
-623.139119	25.495747	0.835802
-626.944022	19.588111	0.840806
-630.587878	20.102472	0.845811
-634.483873	19.491834	0.850816
-637.931491	14.753920	0.855821
-642.148378	18.521426	0.860826
-645.792730	19.229841	0.865830
-649.818334	24.072167	0.870835
-653.481291	9.363606	0.875840
-656.621776	12.400948	0.880845
-660.842937	16.263780	0.885850
-664.615639	13.323416	0.890854
-668.182641	12.534119	0.895859
-671.951375	19.779545	0.900864
-675.806134	18.414962	0.905869
-679.743156	22.281308	0.910874
-683.285470	16.459533	0.915878
-687.450594	16.079631	0.920883
-691.046564	10.129260	0.925888
-694.594841	10.163277	0.930893
-698.451901	21.872709	0.935898
-701.752960	12.455053	0.940902
-705.892695	18.452612	0.945907
-709.723106	15.926791	0.950912
-713.102395	8.368140	0.955917
-717.389007	22.760649	0.960922
-721.095641	11.329556	0.965926
-725.143768	22.211760	0.970931
-728.784722	15.295722	0.975936
-732.249575	11.295515	0.980941
-736.322046	14.472442	0.985946
-739.581360	3.073971	0.990950
-743.165927	19.910384	0.995955
-747.257343	15.734385	1.000960
-751.035081	12.142154	1.005965
-754.854590	17.128320	1.010970
-758.561280	11.112178	1.015974
-762.325807	18.503714	1.020979
-765.948610	27.178233	1.025984
-769.829271	25.508883	1.030989
-773.879506	26.099452	1.035994
-777.388343	18.678284	1.040998
-781.317420	11.645970	1.046003
-785.030685	28.966609	1.051008
-788.637026	23.440639	1.056013
-792.460273	28.501576	1.061018
-796.024287	18.905329	1.066022
-799.715570	19.424377	1.071027
-803.753811	21.585191	1.076032
-807.100484	19.635022	1.081037
-811.613671	24.979722	1.086042
-815.220985	15.989631	1.091046
-818.841832	22.784317	1.096051
-822.416806	18.741927	1.101056
-825.902169	7.061195	1.106061
-830.421548	26.467611	1.111066
-833.987320	10.200096	1.116070
-837.863462	21.930133	1.121075
-841.146110	15.754882	1.126080
-844.791780	16.198904	1.131085
-848.632139	14.431787	1.136090
-852.426176	16.995161	1.141094
-856.590396	23.717506	1.146099
-860.535553	8.247073	1.151104
-864.030287	18.465480	1.156109
-867.622495	19.334622	1.161114
-871.517923	16.772158	1.166118
-874.874297	12.764285	1.171123
-879.316183	20.981752	1.176128
-882.679141	7.770929	1.181133
-886.739488	15.791799	1.186138
-889.960819	16.114437	1.191142
-893.711685	16.070764	1.196147
-897.788926	14.901380	1.201152
-901.620882	18.699252	1.206157
-905.589664	25.341552	1.211162
-909.093231	16.737120	1.216166
-912.550389	8.610945	1.221171
-916.615725	9.822295	1.226176
-920.483623	3.179386	1.231181
-924.263739	15.955408	1.236186
-928.054902	10.323609	1.241190
-931.741710	23.343330	1.246195
-935.226147	16.091964	1.251200
-938.405772	12.350793	1.256205
-943.032410	17.734375	1.261210
-946.896848	3.435406	1.266214
-950.366149	11.640970	1.271219
-954.077033	19.516193	1.276224
-957.425412	15.272214	1.281229
-961.662262	10.697264	1.286234
-965.333122	2.267905	1.291238
-969.471766	17.318360	1.296243
-973.187588	17.705995	1.301248
-976.847514	12.702948	1.306253
-980.501491	20.763062	1.311258
-984.316069	21.544948	1.316262
-988.105327	13.355312	1.321267
-992.046964	20.761329	1.326272
-995.319149	13.386235	1.331277
-999.390355	20.265822	1.336282
-1003.000336	24.739512	1.341286
-1006.894378	19.165293	1.346291
-1010.932695	18.166487	1.351296
-1014.416094	18.781925	1.356301
-1018.067274	21.833611	1.361306
-1021.841152	13.803986	1.366310
-1025.687473	20.787989	1.371315
-1029.724132	23.067197	1.376320
-1033.376003	15.678773	1.381325
-1036.742995	14.876972	1.386330
-1040.528336	9.255469	1.391334
-1044.147134	11.857346	1.396339
-1048.444160	18.971814	1.401344
-1052.309405	12.071680	1.406349
-1056.174351	17.067164	1.411354
-1059.356059	8.988618	1.416358
-1062.919851	6.939519	1.421363
-1066.706197	22.296456	1.426368
-1070.563358	13.740958	1.431373
-1074.756565	12.126844	1.436378
-1078.194527	15.940817	1.441382
-1082.123875	12.690328	1.446387
-1086.069382	18.297944	1.451392
-1089.549156	2.010811	1.456397
-1093.628624	16.343999	1.461402
-1097.244060	10.111983	1.466406
-1100.827983	9.805413	1.471411
-1104.495263	9.472762	1.476416
-1108.309037	9.926739	1.481421
-1112.163999	12.161252	1.486426
-1116.202970	8.819558	1.491430
-1119.471078	9.949450	1.496435
-1123.623678	7.679273	1.501440
-1127.212894	5.604382	1.506445
-1130.868163	13.787914	1.511450
-1134.736274	6.609285	1.516454
-1138.398638	8.857179	1.521459
-1142.607126	10.769860	1.526464
-1146.007328	6.414615	1.531469
-1149.896433	11.095592	1.536474
-1153.652160	5.950478	1.541478
-1157.405048	-2.105915	1.546483
-1160.928372	12.948890	1.551488
-1164.419287	-1.500895	1.556493
-1168.535569	5.479213	1.561498
-1172.436903	-3.059567	1.566502
-1176.309697	3.687645	1.571507
-1180.082185	5.707238	1.576512
-1183.670823	4.020244	1.581517
-1187.110040	8.230358	1.586522
-1191.075610	7.972377	1.591526
-1195.202602	8.214860	1.596531
-1198.743553	15.145540	1.601536
-1202.260190	8.480026	1.606541
-1205.881815	11.571420	1.611546
-1209.581105	-7.242730	1.616550
-1213.607233	-0.925052	1.621555
-1218.048711	7.937880	1.626560
-1221.442287	6.408952	1.631565
-1225.372262	8.564196	1.636570
-1228.568807	-0.818917	1.641574
-1232.046590	7.828332	1.646579
-1236.191118	8.772230	1.651584
-1239.866328	7.091293	1.656589
-1244.082991	12.040867	1.661594
-1247.899293	14.337219	1.666598
-1251.288524	2.608685	1.671603
-1255.218855	4.313062	1.676608
-1258.479450	-0.379718	1.681613
-1262.719318	15.185684	1.686618
-1266.504245	8.468599	1.691622
-1270.476221	12.065559	1.696627
-1274.082408	4.512545	1.701632
-1277.501924	2.115864	1.706637
-1281.454341	2.116111	1.711642
-1285.128297	3.008436	1.716646
-1288.825335	12.324744	1.721651
-1292.861141	6.862019	1.726656
-1296.381646	-5.660648	1.731661
-1300.430390	8.855588	1.736666
-1304.131545	4.462026	1.741670
-1307.567423	-4.661904	1.746675
-1311.565215	4.846063	1.751680
-1314.960977	-2.825709	1.756685
-1318.871409	19.153644	1.761690
-1322.846186	-2.012999	1.766694
-1326.397045	-10.945040	1.771699
-1330.474546	-7.204946	1.776704
-1334.298311	-1.685798	1.781709
-1337.921850	23.532204	1.786714
-1341.386307	10.587496	1.791718
-1345.029043	10.585586	1.796723
-1349.246516	10.074909	1.801728
-1352.737743	11.475791	1.806733
-1356.544980	19.701332	1.811738
-1360.730879	9.574834	1.816742
-1364.344088	5.752297	1.821747
-1368.231113	6.776626	1.826752
-1371.331495	-3.121523	1.831757
-1375.711772	12.632109	1.836762
-1379.272412	9.917576	1.841766
-1382.951345	15.498771	1.846771
-1386.775006	19.693455	1.851776
-1390.280688	8.210845	1.856781
-1394.363222	9.441545	1.861786
-1397.968229	10.468079	1.866790
-1401.690078	5.486680	1.871795
-1405.484483	19.620203	1.876800
-1408.899819	12.792154	1.881805
-1413.203381	17.454766	1.886810
-1416.957353	-1.233576	1.891814
-1420.725386	2.770918	1.896819
-1424.613182	13.734221	1.901824
-1428.251641	13.422699	1.906829
-1432.115084	14.534815	1.911834
-1435.524747	0.236463	1.916838
-1439.323691	7.065306	1.921843
-1442.974563	14.095937	1.926848
-1446.886702	4.797762	1.931853
-1450.846547	17.035686	1.936858
-1454.318941	7.624538	1.941862
-1458.066078	-0.099552	1.946867
-1462.037062	18.649322	1.951872
-1465.724313	9.069184	1.956877
-1469.843870	26.553600	1.961882
-1473.140602	12.502122	1.966886
-1476.812844	7.363106	1.971891
-1480.582767	18.236668	1.976896
-1484.236659	12.307886	1.981901
-1488.563654	11.628937	1.986906
-1492.331146	12.093480	1.991910
-1495.798497	19.864297	1.996915
-1499.805139	18.066175	2.006912
-1500.726960	6.651885	2.016909
-1498.374230	12.907850	2.026906
-1495.375331	16.137896	2.036902
-1492.938973	12.375318	2.046899
-1491.488327	17.574246	2.056896
-1489.607982	12.691310	2.066893
-1487.673356	15.441309	2.076890
-1485.509963	-0.606769	2.086886
-1483.826936	7.115838	2.096883
-1481.933824	7.347911	2.106880
-1479.896679	5.490210	2.116877
-1478.126517	11.211102	2.126874
-1476.130696	6.500728	2.136870
-1474.311461	19.294902	2.146867
-1472.482902	10.717872	2.156864
-1470.725043	8.532292	2.166861
-1468.515345	12.622910	2.176858
-1466.341740	9.537130	2.186854
-1464.685184	5.561574	2.196851
-1462.813574	8.466937	2.206848
-1461.014818	1.595112	2.216845
-1459.198415	10.523149	2.226842
-1457.202711	6.458558	2.236838
-1455.613026	12.918850	2.246835
-1453.409253	6.972114	2.256832
-1451.641349	9.410965	2.266829
-1449.647732	12.337855	2.276826
-1447.964600	-1.205026	2.286822
-1445.839254	6.236802	2.296819
-1443.989123	5.692680	2.306816
-1442.236186	4.298912	2.316813
-1440.391044	7.753235	2.326810
-1438.713374	1.464462	2.336806
-1436.682183	2.430732	2.346803
-1434.227845	8.417881	2.356800
-1432.719011	9.096760	2.366797
-1430.964311	8.920011	2.376794
-1429.376697	5.677051	2.386790
-1427.054135	0.214975	2.396787
-1425.109666	0.483080	2.406784
-1423.303699	11.459007	2.416781
-1421.465155	3.481960	2.426778
-1419.759889	6.786600	2.436774
-1417.931026	17.199958	2.446771
-1415.974376	15.023641	2.456768
-1413.802711	9.004717	2.466765
-1411.961752	17.017873	2.476762
-1410.116558	19.872253	2.486758
-1408.272627	18.607617	2.496755
-1406.446399	13.840770	2.506752
-1404.577747	20.150659	2.516749
-1403.041190	13.393474	2.526746
-1400.753003	15.823276	2.536742
-1398.894003	13.807861	2.546739
-1396.911197	17.410699	2.556736
-1395.369063	16.926975	2.566733
-1393.077698	19.618367	2.576730
-1391.459933	10.310977	2.586726
-1389.739733	9.846116	2.596723
-1387.360413	8.216330	2.606720
-1385.794163	11.469047	2.616717
-1383.935182	13.470240	2.626714
-1382.322043	13.785108	2.636710
-1379.994924	8.843365	2.646707
-1378.232653	6.845030	2.656704
-1376.675035	13.632601	2.666701
-1374.448062	15.996445	2.676698
-1372.516114	15.846626	2.686694
-1370.870844	10.234092	2.696691
-1368.751419	9.236419	2.706688
-1366.910491	13.465116	2.716685
-1365.185439	9.814956	2.726682
-1363.134911	19.787117	2.736678
-1361.280990	5.672237	2.746675
-1359.682982	13.566443	2.756672
-1357.813182	10.712541	2.766669
-1355.699648	6.831264	2.776666
-1353.985836	14.373801	2.786662
-1351.659941	7.239258	2.796659
-1350.123741	15.392826	2.806656
-1348.268782	20.661336	2.816653
-1346.093316	17.989025	2.826650
-1344.499787	17.170286	2.836646
-1342.673311	9.817290	2.846643
-1340.696904	18.416686	2.856640
-1338.707113	8.001422	2.866637
-1337.066478	21.035880	2.876634
-1335.381815	14.798152	2.886630
-1333.036204	17.218832	2.896627
-1331.322361	13.039996	2.906624
-1329.458424	18.507598	2.916621
-1327.499451	16.165203	2.926618
-1325.677960	14.315312	2.936614
-1323.627898	12.624615	2.946611
-1322.208164	17.868079	2.956608
-1319.786957	14.319667	2.966605
-1318.165454	12.964396	2.976602
-1316.417119	16.405901	2.986598
-1314.565772	20.626661	2.996595
-1312.552494	15.381550	3.006592
-1310.650848	13.989339	3.016589
-1308.605435	12.428865	3.026586
-1307.113839	9.959201	3.036582
-1304.970496	9.646136	3.046579
-1303.143244	14.162848	3.056576
-1301.538287	15.109045	3.066573
-1299.477478	14.764987	3.076570
-1297.732030	14.472985	3.086566
-1295.526741	16.601972	3.096563
-1293.631484	17.994313	3.106560
-1291.884774	17.132147	3.116557
-1290.003007	15.946807	3.126554
-1288.574443	14.480339	3.136550
-1286.079058	19.921124	3.146547
-1284.282832	14.721827	3.156544
-1282.470588	13.260268	3.166541
-1280.625868	17.352651	3.176538
-1278.703698	14.796725	3.186534
-1276.853440	17.879338	3.196531
-1275.097459	5.761647	3.206528
-1273.061837	12.633838	3.216525
-1271.272880	15.086831	3.226522
-1269.392484	7.943140	3.236518
-1267.315291	9.129554	3.246515
-1265.601592	7.769038	3.256512
-1263.797738	3.626369	3.266509
-1262.155121	11.530879	3.276506
-1260.089920	17.692604	3.286502
-1258.073367	16.130477	3.296499
-1256.132626	13.942627	3.306496
-1254.219833	12.791821	3.316493
-1252.498275	8.314982	3.326490
-1250.664156	15.772041	3.336486
-1248.669501	12.348801	3.346483
-1246.969361	10.032105	3.356480
-1244.706263	8.661047	3.366477
-1243.060241	13.009455	3.376474
-1241.355526	14.825466	3.386470
-1239.208340	9.205324	3.396467
-1237.741698	11.758867	3.406464
-1235.513589	17.433521	3.416461
-1233.929470	23.309123	3.426458
-1231.692852	19.844018	3.436454
-1229.857085	19.191845	3.446451
-1227.991899	16.583502	3.456448
-1226.273514	15.034381	3.466445
-1224.502499	14.072066	3.476442
-1222.545931	17.900299	3.486438
-1220.595834	16.980379	3.496435
-1218.571664	21.887208	3.506432
-1216.858859	19.259049	3.516429
-1215.005074	14.756339	3.526426
-1213.008396	16.440395	3.536422
-1211.250262	8.515832	3.546419
-1209.277094	13.061375	3.556416
-1207.567177	16.220184	3.566413
-1205.549426	14.141624	3.576410
-1203.465878	15.846523	3.586406
-1201.758025	12.519737	3.596403
-1199.838106	11.584138	3.606400
-1198.247630	21.907957	3.616397
-1196.287109	15.510924	3.626394
-1194.391394	13.653994	3.636390
-1192.283564	9.274854	3.646387
-1190.527487	14.646157	3.656384
-1188.978374	14.810362	3.666381
-1187.049996	9.877343	3.676378
-1184.938929	20.252077	3.686374
-1182.861534	17.202471	3.696371
-1181.097132	10.164240	3.706368
-1179.258100	19.090489	3.716365
-1177.503900	15.416850	3.726362
-1175.520703	12.887557	3.736358
-1173.587328	20.172497	3.746355
-1171.999089	11.275727	3.756352
-1170.028967	15.302351	3.766349
-1167.954536	21.990027	3.776346
-1165.846882	17.342530	3.786342
-1164.445095	18.458690	3.796339
-1162.308378	11.248804	3.806336
-1160.470043	9.483183	3.816333
-1158.815953	14.264549	3.826330
-1157.026836	9.248050	3.836326
-1154.554862	3.072367	3.846323
-1152.902395	11.651137	3.856320
-1151.123181	10.812296	3.866317
-1149.228579	11.690155	3.876314
-1147.580866	10.537638	3.886310
-1145.584537	13.183330	3.896307
-1143.570753	16.211473	3.906304
-1141.629250	8.287618	3.916301
-1140.001879	6.457875	3.926298
-1138.089604	12.467348	3.936294
-1136.104446	10.357749	3.946291
-1134.356088	12.809452	3.956288
-1132.524195	11.692213	3.966285
-1130.274971	7.731006	3.976282
-1128.560337	7.834037	3.986278
-1126.978326	16.550411	3.996275
-1124.865429	13.536227	4.006272
-1122.701414	9.828644	4.016269
-1121.115168	14.677731	4.026266
-1119.368066	8.393845	4.036262
-1117.363916	9.618921	4.046259
-1115.300096	20.329687	4.056256
-1113.806180	17.881873	4.066253
-1111.745911	14.580873	4.076250
-1110.043795	18.208346	4.086246
-1107.734895	15.773838	4.096243
-1106.143487	19.180617	4.106240
-1104.144895	19.408758	4.116237
-1102.757365	13.959198	4.126234
-1100.324141	10.896951	4.136230
-1098.463904	9.001566	4.146227
-1096.738119	6.270371	4.156224
-1094.806684	6.184019	4.166221
-1093.137328	7.434252	4.176218
-1090.872117	5.906697	4.186214
-1089.085863	7.929239	4.196211
-1087.718818	10.631437	4.206208
-1085.670585	12.823642	4.216205
-1083.533137	7.776739	4.226202
-1081.606086	12.208202	4.236198
-1079.955304	11.419957	4.246195
-1077.848386	13.804876	4.256192
-1075.997324	5.612923	4.266189
-1074.206607	9.723588	4.276186
-1072.246351	5.478677	4.286182
-1070.321583	9.979985	4.296179
-1068.526938	2.172830	4.306176
-1066.762656	14.829336	4.316173
-1064.793308	15.256387	4.326170
-1062.870252	7.910246	4.336166
-1061.229370	7.881447	4.346163
-1059.265838	0.198857	4.356160
-1057.259038	6.190123	4.366157
-1055.387145	1.008889	4.376154
-1053.553933	9.405680	4.386150
-1051.720247	3.722168	4.396147
-1049.536534	2.556615	4.406144
-1048.116417	8.349640	4.416141
-1046.204515	6.109735	4.426138
-1044.152409	4.690516	4.436134
-1042.324151	3.787074	4.446131
-1040.315446	3.650515	4.456128
-1038.550133	4.388101	4.466125
-1036.930042	7.105116	4.476122
-1034.950816	10.339397	4.486118
-1032.998394	5.497384	4.496115
-1031.017759	6.691561	4.506112
-1029.281093	12.042415	4.516109
-1027.240809	14.336992	4.526106
-1025.128122	10.552447	4.536102
-1023.509695	9.963615	4.546099
-1021.917172	12.097717	4.556096
-1019.876983	0.095777	4.566093
-1017.658908	8.641034	4.576090
-1016.084208	15.958219	4.586086
-1014.168759	9.090144	4.596083
-1012.419832	4.751191	4.606080
-1010.424952	1.918605	4.616077
-1008.514840	5.705508	4.626074
-1006.786914	1.620957	4.636070
-1004.525201	5.337424	4.646067
-1002.918352	6.851915	4.656064
-1000.917972	2.011731	4.666061
-999.094142	8.777533	4.676058
-997.703261	9.772388	4.686054
-995.303344	6.660314	4.696051
-993.460617	8.077093	4.706048
-991.654072	3.416327	4.716045
-989.909318	2.221560	4.726042
-987.744137	1.523212	4.736038
-986.058048	0.318883	4.746035
-984.296661	6.951007	4.756032
-982.346858	2.401542	4.766029
-980.361464	6.138538	4.776026
-978.544688	6.984775	4.786022
-976.409544	0.897868	4.796019
-974.698617	2.518886	4.806016
-972.836924	7.355608	4.816013
-970.929771	4.308149	4.826010
-969.237706	4.146500	4.836006
-967.326031	5.301236	4.846003
-965.296481	7.109717	4.856000
-963.594597	3.157247	4.865997
-961.452516	0.358002	4.875994
-959.744057	9.685824	4.885990
-958.083590	3.985870	4.895987
-955.838665	7.657706	4.905984
-954.243389	13.026493	4.915981
-952.411579	7.520183	4.925978
-950.388635	13.608438	4.935974
-948.562729	11.036592	4.945971
-946.495432	9.763440	4.955968
-944.673906	13.913494	4.965965
-942.951550	18.385705	4.975962
-940.963489	14.155396	4.985958
-938.744798	10.486599	4.995955
-937.371702	11.402234	5.005952
-935.429702	11.248012	5.015949
-933.535606	9.337867	5.025946
-931.779259	12.538407	5.035942
-929.911556	11.679267	5.045939
-927.793565	14.547265	5.055936
-925.700492	8.883943	5.065933
-924.238132	8.912204	5.075930
-922.161106	13.019845	5.085926
-920.402966	12.525580	5.095923
-918.479085	14.613089	5.105920
-916.509271	4.469739	5.115917
-914.615721	8.699873	5.125914
-913.028287	8.455526	5.135910
-910.937909	9.689100	5.145907
-908.910510	12.486341	5.155904
-907.427334	8.104691	5.165901
-905.592204	13.240967	5.175898
-903.356424	13.901857	5.185894
-901.483289	5.455458	5.195891
-899.577940	9.229009	5.205888
-897.867860	6.408892	5.215885
-895.886849	9.065148	5.225882
-894.181343	2.274939	5.235878
-892.294144	14.199884	5.245875
-890.240241	2.912646	5.255872
-888.417579	7.804626	5.265869
-886.522351	8.916271	5.275866
-884.517330	7.182630	5.285862
-883.009678	5.189054	5.295859
-881.215765	5.003291	5.305856
-878.910538	3.575324	5.315853
-877.220816	7.629668	5.325850
-875.339437	6.801541	5.335846
-873.258477	6.178338	5.345843
-871.717140	4.593043	5.355840
-869.716673	10.118155	5.365837
-867.879153	7.591879	5.375834
-865.970943	12.684927	5.385830
-863.700758	9.873180	5.395827
-862.099272	11.278108	5.405824
-860.534861	5.442002	5.415821
-858.246820	7.447662	5.425818
-856.536866	3.231884	5.435814
-854.750998	13.370007	5.445811
-852.809195	4.473742	5.455808
-851.125766	13.715664	5.465805
-849.128311	9.660760	5.475802
-847.158152	16.504351	5.485798
-845.109812	17.203156	5.495795
-843.494118	13.304014	5.505792
-841.544187	10.661898	5.515789
-839.593188	22.309873	5.525786
-837.697072	14.652429	5.535782
-835.926530	13.028938	5.545779
-833.982414	9.610959	5.555776
-832.324115	6.057102	5.565773
-830.268383	3.244934	5.575770
-828.371131	9.943886	5.585766
-826.754879	0.643392	5.595763
-824.478988	4.905638	5.605760
-822.784325	-3.516909	5.615757
-820.945948	10.785771	5.625754
-819.221304	14.373551	5.635750
-817.173464	6.756606	5.645747
-815.141018	6.646443	5.655744
-813.089313	12.802855	5.665741
-811.445280	9.311288	5.675738
-809.604769	16.971382	5.685734
-807.732772	13.583897	5.695731
-806.093486	2.741922	5.705728
-803.995240	15.507905	5.715725
-802.284143	10.679382	5.725722
-800.336675	21.281174	5.735718
-798.518185	22.269377	5.745715
-796.534777	20.010344	5.755712
-794.484061	19.581507	5.765709
-792.616361	13.280142	5.775706
-790.964860	17.189093	5.785702
-788.949093	13.693384	5.795699
-787.097789	18.929801	5.805696
-785.164172	11.807951	5.815693
-783.560924	13.283701	5.825690
-781.484108	17.580970	5.835686
-779.534422	17.986144	5.845683
-777.959102	9.385335	5.855680
-775.917415	15.769162	5.865677
-773.806543	16.276466	5.875674
-772.123271	10.271422	5.885670
-770.434480	4.486540	5.895667
-768.314899	16.357094	5.905664
-766.334414	9.478807	5.915661
-764.503964	17.511581	5.925658
-762.640628	11.168307	5.935654
-760.921023	12.616003	5.945651
-758.881290	13.832546	5.955648
-757.194117	2.218778	5.965645
-755.248241	10.188900	5.975642
-753.434207	11.588353	5.985638
-751.353609	9.688016	5.995635
-749.912346	11.788065	6.005632
-747.843924	10.107559	6.015629
-745.804414	4.655042	6.025626
-743.820322	3.837444	6.035622
-742.091470	6.317829	6.045619
-740.074420	9.390017	6.055616
-738.424407	12.936105	6.065613
-736.572237	11.880663	6.075610
-734.560521	14.618991	6.085606
-732.858487	11.514500	6.095603
-730.631283	12.731107	6.105600
-728.886610	12.278607	6.115597
-727.038804	15.605211	6.125594
-725.479662	20.293140	6.135590
-723.336142	17.806486	6.145587
-721.197655	19.335685	6.155584
-719.814969	15.437545	6.165581
-717.786707	15.497072	6.175578
-715.623497	16.356045	6.185574
-713.885015	17.047642	6.195571
-712.294685	17.481878	6.205568
-710.284606	15.959141	6.215565
-708.021267	16.780016	6.225562
-706.419862	15.205752	6.235558
-704.638111	12.832186	6.245555
-702.479235	5.939652	6.255552
-700.797832	13.980508	6.265549
-699.204251	7.295145	6.275546
-697.156763	1.940861	6.285542
-695.229451	12.566492	6.295539
-693.384285	10.866448	6.305536
-691.195915	14.555480	6.315533
-689.508253	10.897557	6.325530
-687.718403	12.498284	6.335526
-685.788970	11.575790	6.345523
-684.012766	15.605412	6.355520
-681.985457	14.315195	6.365517
-680.265152	7.816426	6.375514
-678.171461	9.899107	6.385510
-676.397182	14.562166	6.395507
-674.578710	17.066176	6.405504
-672.871431	10.904210	6.415501
-670.870238	17.684586	6.425498
-668.802730	9.573586	6.435494
-667.070051	15.146409	6.445491
-665.232707	11.256175	6.455488
-663.263130	2.576652	6.465485
-661.452824	-3.034952	6.475482
-659.193901	-1.529679	6.485478
-657.664737	4.633003	6.495475
-655.757346	13.362484	6.505472
-654.041044	8.577437	6.515469
-651.826772	4.608043	6.525466
-650.147014	13.721249	6.535462
-648.459964	5.708948	6.545459
-646.314218	9.160109	6.555456
-644.613173	3.242305	6.565453
-642.659948	6.380037	6.575450
-640.844735	7.223630	6.585446
-639.045135	2.428444	6.595443
-636.779786	4.581625	6.605440
-634.973612	8.248094	6.615437
-633.191899	3.790488	6.625434
-631.427741	3.966492	6.635430
-629.760433	0.573954	6.645427
-627.719322	1.690922	6.655424
-625.602380	-0.799292	6.665421
-623.545567	8.411578	6.675418
-622.303057	13.148586	6.685414
-620.197829	7.761454	6.695411
-618.477078	5.522427	6.705408
-616.258894	2.679748	6.715405
-614.588774	5.108037	6.725402
-612.740914	2.329261	6.735398
-610.568984	9.815004	6.745395
-608.731123	6.381021	6.755392
-607.187311	8.393728	6.765389
-605.242582	6.939936	6.775386
-603.112255	6.743270	6.785382
-601.250593	5.313804	6.795379
-599.496194	8.723324	6.805376
-597.579450	7.057705	6.815373
-595.420528	2.857217	6.825370
-594.159514	10.543758	6.835366
-592.132811	6.238085	6.845363
-590.036965	14.601222	6.855360
-588.129407	-2.276848	6.865357
-586.315930	6.049295	6.875354
-584.576689	11.952695	6.885350
-582.573030	12.223100	6.895347
-580.796221	8.972566	6.905344
-578.825265	11.193358	6.915341
-576.983582	12.448014	6.925338
-575.000459	9.775546	6.935334
-573.219811	14.320834	6.945331
-571.386393	12.324354	6.955328
-569.513407	14.008203	6.965325
-567.703362	2.256502	6.975322
-565.790538	4.810258	6.985318
-564.030211	6.096865	6.995315
-561.816996	13.446596	7.005312
-560.185400	10.511362	7.015309
-558.162940	3.670739	7.025306
-556.303347	6.373525	7.035302
-554.366005	6.285093	7.045299
-552.459267	15.919462	7.055296
-550.607693	13.774841	7.065293
-548.810814	6.477651	7.075290
-547.184334	7.877226	7.085286
-545.305733	11.379048	7.095283
-543.033397	11.600255	7.105280
-541.382858	10.908732	7.115277
-539.601009	7.010087	7.125274
-537.640363	11.141409	7.135270
-535.729638	5.329123	7.145267
-533.840685	6.858879	7.155264
-531.838779	10.999404	7.165261
-529.963847	11.841438	7.175258
-528.287963	6.035091	7.185254
-526.639029	9.287838	7.195251
-524.502471	18.776585	7.205248
-522.330706	12.900508	7.215245
-520.664590	9.811372	7.225242
-518.506844	13.041275	7.235238
-517.187988	6.433057	7.245235
-515.149381	6.746882	7.255232
-513.272103	11.747285	7.265229
-511.203139	15.101897	7.275226
-509.550919	11.265027	7.285222
-507.315125	6.643410	7.295219
-505.669778	16.966905	7.305216
-504.009867	2.809348	7.315213
-501.889340	9.021370	7.325210
-500.254470	12.077446	7.335206
-498.082394	8.803312	7.345203
-496.184336	12.068396	7.355200
-494.467645	9.959571	7.365197
-492.479752	5.677544	7.375194
-490.567658	2.487569	7.385190
-488.451443	2.111689	7.395187
-487.056136	11.076254	7.405184
-485.317175	4.781465	7.415181
-483.233630	14.877107	7.425178
-481.186671	7.031628	7.435174
-479.452589	4.577422	7.445171
-477.378878	13.809421	7.455168
-475.607906	15.508059	7.465165
-473.851372	18.314211	7.475162
-471.898432	18.523340	7.485158
-469.783390	16.723526	7.495155
-468.080746	11.958151	7.505152
-466.513805	10.890050	7.515149
-464.256804	18.116053	7.525146
-462.657197	15.359665	7.535142
-460.747057	13.358910	7.545139
-458.532835	13.341596	7.555136
-457.042396	8.409601	7.565133
-455.118940	12.065380	7.575130
-453.193808	5.881400	7.585126
-451.305592	10.382766	7.595123
-449.249140	17.083471	7.605120
-447.546659	10.529279	7.615117
-445.661958	10.692487	7.625114
-443.505023	17.075588	7.635110
-441.806447	14.107630	7.645107
-440.050211	18.069586	7.655104
-438.144819	17.654788	7.665101
-436.173247	13.721182	7.675098
-434.396793	11.653378	7.685094
-432.603861	17.710951	7.695091
-430.749779	10.731530	7.705088
-428.661889	13.150083	7.715085
-426.913877	11.483122	7.725082
-424.981804	22.360871	7.735078
-423.170742	20.737525	7.745075
-421.186839	10.715428	7.755072
-419.340208	16.500766	7.765069
-417.673895	7.803532	7.775066
-415.596718	14.534114	7.785062
-413.638577	21.681584	7.795059
-411.779357	7.334360	7.805056
-409.820334	16.908408	7.815053
-408.053704	18.034662	7.825050
-406.571899	22.177826	7.835046
-404.443742	18.062932	7.845043
-402.238904	16.599348	7.855040
-400.646363	17.151856	7.865037
-398.895926	18.514375	7.875034
-396.622633	13.891602	7.885030
-395.038757	16.657491	7.895027
-393.127749	16.096577	7.905024
-391.302175	16.438207	7.915021
-389.209978	13.307968	7.925018
-387.301320	9.090776	7.935014
-385.547231	14.993544	7.945011
-383.841554	13.453367	7.955008
-381.997174	17.344456	7.965005
-380.246819	10.643723	7.975002
-378.020898	17.060081	7.984998
-376.163231	15.642477	7.994995
-374.284482	12.944204	8.004992
-372.459149	14.057954	8.014989
-370.349100	12.516379	8.024986
-368.431813	14.024378	8.034982
-366.970138	7.717096	8.044979
-365.099907	14.453926	8.054976
-362.755507	15.693222	8.064973
-361.106823	2.972725	8.074970
-359.483447	16.378636	8.084966
-357.394520	10.414877	8.094963
-355.541620	15.447726	8.104960
-353.721095	13.226110	8.114957
-351.960841	14.160801	8.124954
-350.294611	9.365004	8.134950
-348.154181	12.570991	8.144947
-345.975006	19.605868	8.154944
-344.290236	13.788743	8.164941
-342.285513	20.619381	8.174938
-340.638451	15.652972	8.184934
-338.624568	12.367918	8.194931
-337.045432	12.377899	8.204928
-334.752991	9.807813	8.214925
-333.153179	18.994038	8.224922
-331.180922	16.470334	8.234918
-329.163377	22.564764	8.244915
-327.687307	12.278031	8.254912
-325.661354	8.166892	8.264909
-323.641606	13.506272	8.274906
-321.458361	16.231789	8.284902
-319.913034	17.548167	8.294899
-318.014392	14.139427	8.304896
-316.306430	16.625049	8.314893
-314.349513	12.003911	8.324890
-312.281066	11.222148	8.334886
-310.559708	15.584489	8.344883
-308.763354	11.737371	8.354880
-306.548267	5.815091	8.364877
-304.731624	15.429331	8.374874
-302.871530	14.393482	8.384870
-301.455967	4.326416	8.394867
-299.570806	15.628586	8.404864
-297.554573	10.985362	8.414861
-295.601454	18.676868	8.424858
-293.276037	8.933489	8.434854
-291.887466	8.058176	8.444851
-290.049845	18.068535	8.454848
-288.148596	15.054119	8.464845
-285.917273	16.936773	8.474842
-284.064356	13.705876	8.484838
-282.394717	13.657238	8.494835
-280.701482	13.434317	8.504832
-278.716137	18.040321	8.514829
-276.430581	7.865973	8.524826
-274.710110	11.849553	8.534822
-273.454047	15.924631	8.544819
-271.402556	20.992166	8.554816
-268.915450	13.315001	8.564813
-267.266078	7.495682	8.574810
-265.445479	18.089805	8.584807
-263.858092	20.444719	8.594803
-261.445948	17.462454	8.604800
-259.897140	18.276235	8.614797
-258.075064	14.530831	8.624794
-256.309126	14.970500	8.634791
-254.024191	21.050739	8.644787
-252.248209	18.616843	8.654784
-250.380562	15.869911	8.664781
-248.766740	17.685378	8.674778
-246.845695	11.347470	8.684775
-245.066776	19.325761	8.694771
-243.318652	23.731250	8.704768
-240.993436	16.946748	8.714765
-238.912573	19.983933	8.724762
-237.306704	18.129803	8.734759
-235.554311	17.453809	8.744755
-233.484510	18.992837	8.754752
-231.957202	22.238372	8.764749
-229.857202	17.348156	8.774746
-227.894612	17.156490	8.784743
-226.195729	20.497797	8.794739
-224.085177	14.477010	8.804736
-222.403262	16.625822	8.814733
-220.461614	7.868973	8.824730
-218.302673	13.287282	8.834727
-216.527851	7.223774	8.844723
-214.887337	13.387950	8.854720
-213.271830	5.966780	8.864717
-211.022591	5.972526	8.874714
-209.168285	12.078902	8.884711
-207.240998	14.344873	8.894707
-205.412199	7.671208	8.904704
-203.662264	13.828982	8.914701
-201.735518	6.001324	8.924698
-199.978543	17.511928	8.934695
-197.861739	7.572988	8.944691
-195.894460	10.825695	8.954688
-194.142483	17.764693	8.964685
-192.362163	6.327426	8.974682
-190.718501	13.094245	8.984679
-188.728124	14.633356	8.994675
-186.851952	10.175194	9.004672
-184.818281	12.444731	9.014669
-182.716835	13.884021	9.024666
-181.160721	8.741185	9.034663
-179.393616	13.917338	9.044659
-177.341410	10.361047	9.054656
-175.271473	8.203966	9.064653
-173.397670	12.537347	9.074650
-171.797373	6.864860	9.084647
-169.715778	11.712954	9.094643
-168.068173	9.264869	9.104640
-166.161087	14.852885	9.114637
-164.183742	4.813075	9.124634
-162.590871	6.884562	9.134631
-160.431160	11.377584	9.144627
-158.084629	13.815105	9.154624
-156.793712	12.200749	9.164621
-154.809861	7.243874	9.174618
-152.818218	10.158009	9.184615
-151.108076	7.755217	9.194611
-149.322317	18.416576	9.204608
-147.467724	9.484205	9.214605
-145.313354	12.636053	9.224602
-143.329999	13.604770	9.234599
-141.669424	10.418879	9.244595
-139.848199	11.716612	9.254592
-138.013783	10.244480	9.264589
-136.257682	9.673751	9.274586
-134.367387	9.511064	9.284583
-132.150070	12.106590	9.294579
-130.400613	10.678018	9.304576
-128.388025	14.332482	9.314573
-126.593000	13.888174	9.324570
-124.645748	14.769514	9.334567
-123.019774	15.283716	9.344563
-120.936728	16.670736	9.354560
-119.068278	15.583169	9.364557
-117.385879	17.845658	9.374554
-115.491646	21.951631	9.384551
-113.593892	18.309511	9.394547
-111.745323	13.140578	9.404544
-109.589431	11.206668	9.414541
-108.017111	14.751404	9.424538
-106.177466	20.768634	9.434535
-104.145417	16.374078	9.444531
-102.210347	21.495076	9.454528
-100.590011	19.932396	9.464525
-98.646874	22.732746	9.474522
-96.370859	20.785997	9.484519
-94.745961	18.559466	9.494515
-93.031536	26.785008	9.504512
-91.023639	20.014950	9.514509
-88.907949	20.594723	9.524506
-87.397093	14.535519	9.534503
-85.436586	17.094698	9.544499
-83.779104	18.491228	9.554496
-81.722798	15.929049	9.564493
-79.849939	18.836937	9.574490
-77.785941	14.535195	9.584487
-75.882015	8.515917	9.594483
-74.108945	17.884690	9.604480
-72.425305	17.923959	9.614477
-70.246322	21.280363	9.624474
-68.365426	14.718472	9.634471
-66.972735	23.543229	9.644467
-64.608619	22.776083	9.654464
-62.742080	17.219071	9.664461
-60.994192	20.814775	9.674458
-59.117907	15.303577	9.684455
-57.211463	15.705189	9.694451
-55.668394	21.559785	9.704448
-53.356022	23.377628	9.714445
-51.753153	20.962016	9.724442
-49.784246	16.523893	9.734439
-47.879081	22.754921	9.744435
-45.986828	24.033503	9.754432
-44.143340	23.107862	9.764429
-42.384988	22.281063	9.774426
-40.195308	20.018153	9.784423
-38.445111	24.259267	9.794419
-36.887394	21.767187	9.804416
-34.773403	28.713303	9.814413
-32.603198	19.310675	9.824410
-30.800612	19.242582	9.834407
-29.336443	17.398559	9.844403
-27.330429	18.655850	9.854400
-25.450646	20.860079	9.864397
-23.286739	20.006493	9.874394
-21.681583	17.143715	9.884391
-19.984988	20.692372	9.894387
-17.560784	25.976988	9.904384
-15.823824	20.031749	9.914381
-14.167536	17.214501	9.924378
-12.325726	15.829699	9.934375
-10.220712	13.648213	9.944371
-8.423040	16.582361	9.954368
-6.573809	11.446553	9.964365
-4.711242	14.395614	9.974362
-3.347566	38.740661	9.984359
-1.991342	69.484562	9.994355
-0.820980	117.764852	10.004352
0.000000	179.616090	10.009357
0.871910	206.744335	10.014362
1.409410	242.482123	10.019367
1.618749	266.313256	10.024371
2.206123	295.190087	10.029376
2.429244	305.502025	10.034381
2.495170	336.841636	10.039386
3.089374	335.748681	10.044391
2.785682	348.059024	10.049395
3.290317	367.356966	10.054400
3.647683	386.509696	10.059405
3.785318	386.490892	10.064410
3.870197	391.570725	10.069415
3.864811	402.143099	10.074419
3.888292	402.103081	10.079424
4.069397	398.791089	10.084429
3.710021	412.042314	10.089434
3.989508	414.244811	10.094439
3.795895	416.800305	10.099443
3.655384	408.826258	10.104448
4.075843	413.355848	10.109453
4.008872	424.001138	10.114458
4.698970	407.669496	10.119463
4.052814	423.590434	10.124467
3.997385	416.747641	10.129472
4.359233	419.298112	10.134477
3.777796	423.039796	10.139482
4.268855	440.830909	10.144487
4.641019	449.835578	10.149491
4.843458	455.912208	10.154496
4.753054	450.535191	10.159501
4.861500	444.443659	10.164506
4.902169	439.217622	10.169511
4.568616	444.010988	10.174515
4.496609	438.976383	10.179520
4.793525	438.083800	10.184525
4.513121	458.043227	10.189530
4.608850	461.404105	10.194535
4.785307	463.908464	10.199539
4.773678	464.312425	10.204544
4.723234	471.998418	10.209549
4.739486	476.776999	10.214554
5.127511	459.299764	10.219559
5.055421	481.380048	10.224563
5.151373	470.909853	10.229568
5.239866	470.514122	10.234573
5.112263	478.559345	10.239578
5.487009	470.160889	10.244583
5.150061	489.910190	10.249587
5.639589	498.987631	10.254592
5.640269	491.782626	10.259597
5.575796	483.919407	10.264602
5.887658	478.788867	10.269607
5.508880	479.716578	10.274611
5.471704	485.703710	10.279616
5.593318	487.879363	10.284621
5.415915	486.724974	10.289626
5.841740	513.805107	10.294631
5.885478	510.064004	10.299635
6.063145	513.191057	10.304640
6.001066	518.876255	10.309645
5.800931	527.626914	10.314650
6.176321	521.935883	10.319655
6.097515	522.293793	10.324659
6.014494	511.863153	10.329664
6.191215	512.743261	10.334669
5.821994	522.500148	10.339674
6.143167	516.757845	10.344679
6.249628	532.077898	10.349683
6.369982	525.123439	10.354688
6.166671	526.415816	10.359693
5.919200	532.050167	10.364698
6.454136	527.540024	10.369703
6.186458	536.799766	10.374707
5.953486	537.641147	10.379712
6.466320	527.359877	10.384717
6.266431	540.645703	10.389722
6.531418	545.196980	10.394727
6.576407	569.004366	10.399731
6.979827	563.788231	10.404736
7.148784	564.164968	10.409741
6.851388	564.467860	10.414746
6.659949	548.998896	10.419751
6.375098	565.874738	10.424755
6.562687	574.825350	10.429760
6.695907	571.686533	10.434765
6.882254	584.973870	10.439770
6.767990	583.847249	10.444775
6.394455	590.323304	10.449779
7.076379	586.395235	10.454784
7.223423	606.479071	10.459789
7.147407	618.557789	10.464794
7.352265	619.748800	10.469799
7.407823	615.274093	10.474803
7.456925	618.128368	10.479808
7.572457	617.253668	10.484813
7.598099	628.663335	10.489818
7.837109	602.647009	10.494823
7.896112	630.987484	10.499827
7.573012	602.755356	10.504832
7.345444	600.312732	10.509837
7.484953	619.544674	10.514842
7.719743	617.097684	10.519847
7.797797	625.160646	10.524851
7.963209	623.549451	10.529856
7.997753	623.923975	10.534861
7.702967	631.309987	10.539866
7.976875	629.711448	10.544871
7.434363	635.793437	10.549875
8.051246	623.683618	10.554880
8.038662	619.399548	10.559885
7.898160	633.488101	10.564890
8.366277	630.855662	10.569895
8.044069	627.034129	10.574899
8.064244	629.550828	10.579904
8.356492	629.609864	10.584909
8.221284	630.768386	10.589914
8.466969	632.673541	10.594919
8.016855	630.029870	10.599923
8.048036	646.543166	10.604928
8.201748	652.843690	10.609933
8.358722	651.749493	10.614938
8.782813	661.843553	10.619943
8.704963	654.616300	10.624947
8.668216	657.496892	10.629952
9.009480	654.449451	10.634957
8.732058	656.381276	10.639962
9.085204	651.280360	10.644967
8.809140	657.288320	10.649971
9.010202	650.738813	10.654976
8.979525	657.918712	10.659981
9.071221	655.127116	10.664986
9.014667	657.346982	10.669991
9.014074	661.885465	10.674995
8.892107	662.611378	10.680000
8.995726	662.612192	10.685005
8.911652	662.362251	10.690010
9.299710	660.802271	10.695015
9.197082	671.486545	10.700019
9.013172	666.687324	10.705024
9.310158	676.748053	10.710029
9.344906	686.629847	10.715034
9.546812	687.390833	10.720039
9.736086	691.342386	10.725043
9.649776	689.571064	10.730048
9.973932	686.684038	10.735053
9.234113	683.756987	10.740058
9.690721	681.392876	10.745063
9.565039	700.015953	10.750067
9.598955	690.301382	10.755072
9.764531	693.353134	10.760077
9.685451	701.483779	10.765082
10.060612	688.795882	10.770087
10.082871	689.382099	10.775091
9.935604	700.221745	10.780096
9.991523	695.202915	10.785101
10.248328	694.986910	10.790106
10.444985	698.796940	10.795111
10.050203	700.641836	10.800115
10.111325	693.874937	10.805120
10.302367	697.602285	10.810125
9.973240	704.257385	10.815130
10.179439	703.423411	10.820135
10.289605	710.681795	10.825139
10.304477	701.604181	10.830144
10.249746	710.875799	10.835149
10.577290	712.673291	10.840154
10.690741	738.266161	10.845159
10.600204	744.126295	10.850163
10.546885	734.081837	10.855168
11.163530	727.262586	10.860173
10.838574	730.047238	10.865178
11.026846	709.755199	10.870183
10.562142	707.120148	10.875187
10.828265	716.099322	10.880192
10.787482	725.094338	10.885197
10.932009	735.502697	10.890202
11.063058	735.659984	10.895207
10.875290	730.568047	10.900211
10.949174	730.229833	10.905216
11.113975	734.458110	10.910221
11.148878	740.424389	10.915226
11.179037	733.949413	10.920231
10.996392	738.272533	10.925235
11.009876	731.297175	10.930240
11.327012	741.506122	10.935245
11.133474	745.157630	10.940250
11.231088	734.628633	10.945255
11.286388	752.633137	10.950259
11.575620	757.272077	10.955264
11.774350	766.531688	10.960269
11.592036	767.898007	10.965274
12.001959	762.668149	10.970279
11.870449	772.940792	10.975283
11.726282	763.131577	10.980288
11.809359	745.183826	10.985293
11.957771	760.749740	10.990298
12.357235	751.736906	10.995303
11.993511	749.457897	11.000307
12.052611	749.435851	11.005312
11.992558	742.232523	11.010317
12.026334	742.545673	11.015322
12.332946	731.896610	11.020327
11.907844	744.092613	11.025331
12.124160	747.565210	11.030336
12.461774	752.516550	11.035341
11.936070	767.456718	11.040346
12.214474	767.647272	11.045351
12.386062	770.184000	11.050355
12.299717	775.824284	11.055360
12.685351	770.590413	11.060365
12.546538	775.978870	11.065370
12.729965	770.392479	11.070375
12.244694	775.599656	11.075379
12.189098	776.365450	11.080384
12.759569	775.719372	11.085389
12.454245	778.198130	11.090394
12.686516	777.128183	11.095399
12.448409	783.278373	11.100403
12.539745	782.264021	11.105408
12.714748	789.441141	11.110413
12.937979	797.160924	11.115418
13.164056	800.570476	11.120423
13.093952	800.006070	11.125427
13.284209	803.702032	11.130432
13.144237	791.214481	11.135437
13.135773	805.225371	11.140442
13.454633	804.242536	11.145447
13.628027	797.908686	11.150451
13.344502	789.441580	11.155456
13.573574	778.497348	11.160461
13.212182	784.949475	11.165466
13.244354	768.063211	11.170471
13.246054	789.985540	11.175475
13.496207	791.268689	11.180480
13.563999	803.843437	11.185485
13.886374	798.763148	11.190490
14.011787	793.968164	11.195495
13.694800	788.349619	11.200499
13.393505	792.082980	11.205504
13.724718	801.829258	11.210509
13.439295	795.010354	11.215514
14.012824	797.101358	11.220519
13.567926	801.248708	11.225523
13.718958	795.670628	11.230528
13.835220	796.151970	11.235533
13.569675	811.971621	11.240538
13.620262	800.311525	11.245543
14.023920	827.894097	11.250547
13.987427	836.522647	11.255552
14.161261	835.659135	11.260557
14.393160	843.746566	11.265562
14.699876	834.174467	11.270567
14.298428	836.285368	11.275571
14.388175	834.000248	11.280576
14.828722	822.870866	11.285581
14.688983	845.609042	11.290586
14.968121	828.746394	11.295591
14.733719	823.141471	11.300595
14.582406	804.522985	11.305600
14.508546	803.514480	11.310605
14.527892	799.927002	11.315610
14.812153	810.882404	11.320615
14.655790	830.587594	11.325619
14.545694	828.042616	11.330624
14.770981	828.971768	11.335629
14.784401	842.952395	11.340634
15.029544	833.427964	11.345639
15.292619	839.678011	11.350643
15.210251	829.474118	11.355648
15.060251	838.311584	11.360653
15.224303	832.639950	11.365658
15.335244	821.555256	11.370663
15.465448	835.268092	11.375667
15.746734	831.104243	11.380672
15.548790	826.696712	11.385677
15.320254	820.791235	11.390682
15.507411	798.517032	11.395687
15.470331	793.311152	11.400691
15.347641	807.393879	11.405696
15.674887	810.889799	11.410701
15.477606	830.016469	11.415706
15.468843	824.850217	11.420711
15.697113	839.665469	11.425715
15.599752	837.454347	11.430720
15.793109	836.459988	11.435725
15.537328	833.799474	11.440730
15.717581	839.163872	11.445735
15.557954	835.593893	11.450739
15.915946	825.633577	11.455744
15.778094	836.921253	11.460749
15.405951	844.929989	11.465754
15.646354	827.866940	11.470759
16.137276	853.297306	11.475763
15.967693	859.903375	11.480768
16.280925	855.188800	11.485773
15.993629	857.333536	11.490778
16.055907	859.860907	11.495783
16.238616	865.185499	11.500787
16.091585	868.295034	11.505792
16.231158	861.681124	11.510797
16.126685	860.429917	11.515802
16.453151	854.068475	11.520807
16.362328	864.035074	11.525811
16.338614	871.704399	11.530816
17.154017	881.559583	11.535821
17.204054	867.053126	11.540826
17.123567	847.863469	11.545831
17.190983	856.103299	11.550835
17.135566	845.551321	11.555840
17.095659	853.216911	11.560845
16.942356	863.374824	11.565850
17.130812	847.723521	11.570855
17.344762	854.795114	11.575859
16.955496	860.520016	11.580864
17.268416	851.374269	11.585869
17.326784	854.919394	11.590874
17.231998	852.485509	11.595879
17.326614	851.413859	11.600883
17.287293	842.240722	11.605888
17.272030	849.375680	11.610893
16.908729	857.477629	11.615898
17.153631	843.416352	11.620903
17.208273	857.513421	11.625907
17.383900	857.621022	11.630912
17.464502	847.108849	11.635917
17.325137	858.232780	11.640922
17.628054	849.520713	11.645927
17.653947	849.510271	11.650931
17.437546	855.887264	11.655936
17.474464	855.122859	11.660941
17.051881	862.250251	11.665946
17.449579	880.476269	11.670951
17.678524	873.417591	11.675955
17.609156	890.138015	11.680960
17.852209	886.242022	11.685965
17.728746	890.450092	11.690970
17.845736	882.472558	11.695975
17.471335	900.026966	11.700979
18.170055	907.549544	11.705984
18.334696	908.352757	11.710989
18.163170	912.991122	11.715994
18.507011	902.397499	11.720999
18.429470	910.643133	11.726003
18.450398	913.248072	11.731008
18.757252	896.120728	11.736013
18.626222	899.522607	11.741018
18.437576	882.247230	11.746023
18.697022	891.552431	11.751027
18.299330	890.407914	11.756032
18.359560	888.677849	11.761037
18.181842	897.789431	11.766042
18.603835	903.749230	11.771047
18.616195	920.563886	11.776051
18.440374	910.851081	11.781056
18.731921	903.419705	11.786061
18.758353	916.089458	11.791066
19.100970	908.578971	11.796071
18.736397	912.465958	11.801075
18.654144	904.537537	11.806080
18.943727	913.579326	11.811085
18.832241	915.588796	11.816090
19.186770	921.931525	11.821095
19.292970	935.211468	11.826099
19.512767	928.521654	11.831104
19.352690	915.810120	11.836109
18.980888	909.790262	11.841114
19.560265	912.872255	11.846119
19.645555	921.025691	11.851123
19.375190	907.322505	11.856128
19.646322	900.151430	11.861133
19.614159	903.444501	11.866138
19.743837	908.145210	11.871143
19.764610	902.397054	11.876147
19.732712	901.607353	11.881152
20.082300	900.717382	11.886157
19.689333	904.675128	11.891162
19.656407	895.628670	11.896167
19.546948	908.061470	11.901171
19.713201	905.199587	11.906176
20.084806	924.935814	11.911181
20.062970	928.533173	11.916186
20.349661	921.102562	11.921191
20.223822	911.728714	11.926195
20.070531	899.776203	11.931200
20.102838	907.226878	11.936205
20.244222	901.555679	11.941210
20.216953	893.752535	11.946215
20.363228	905.209411	11.951219
20.200778	896.092148	11.956224
20.388677	900.923918	11.961229
20.357245	917.833865	11.966234
20.650678	916.139141	11.971239
20.409666	913.171904	11.976243
20.544273	923.903681	11.981248
20.882888	934.733814	11.986253
20.673579	924.222094	11.991258
20.624851	905.987660	11.996263
20.475691	915.996715	12.001267
20.535754	934.153651	12.006272
20.938568	932.375248	12.011277
20.911615	935.136061	12.016282
21.036883	945.293754	12.021287
21.071434	941.982937	12.026291
20.984999	918.302964	12.031296
20.682676	910.072173	12.036301
20.560089	917.855063	12.041306
20.734746	901.034227	12.046311
20.770653	912.846181	12.051315
20.593659	922.083819	12.056320
21.133914	926.785280	12.061325
20.366624	927.346050	12.066330
20.516984	933.841197	12.071335
20.748054	935.840188	12.076339
20.603332	936.672245	12.081344
20.606962	936.039303	12.086349
20.760401	945.232136	12.091354
20.856756	941.528261	12.096359
20.903850	941.298395	12.101363
20.886307	937.163255	12.106368
21.121533	931.639503	12.111373
20.761117	937.807689	12.116378
21.082663	940.145487	12.121383
21.075423	943.712137	12.126387
20.977988	925.655758	12.131392
20.936417	908.847324	12.136397
20.569856	914.511855	12.141402
20.883865	901.273708	12.146407
20.817218	907.735647	12.151411
20.570611	914.472297	12.156416
20.668759	909.279500	12.161421
20.489814	923.926401	12.166426
20.932050	927.448164	12.171431
20.930016	941.532277	12.176435
20.833839	933.841028	12.181440
20.864096	921.084938	12.186445
20.744153	921.181336	12.191450
20.718398	918.446270	12.196455
20.711242	913.297075	12.201459
21.086426	930.069642	12.206464
21.217546	926.453267	12.211469
20.952379	911.003558	12.216474
21.354124	909.619566	12.221479
21.128273	924.169869	12.226483
21.126320	916.045708	12.231488
21.239492	900.360624	12.236493
20.843285	907.996341	12.241498
20.982086	903.785811	12.246503
20.900265	886.611661	12.251507
20.716298	884.327613	12.256512
20.587858	882.575602	12.261517
20.668713	904.811910	12.266522
20.872605	902.590575	12.271527
20.547556	920.203368	12.276531
20.757770	908.404184	12.281536
21.013515	914.734281	12.286541
20.740769	918.130383	12.291546
20.736845	914.220159	12.296551
21.305849	908.491791	12.301555
20.758334	903.665329	12.306560
20.881565	896.051068	12.311565
21.019744	895.235818	12.316570
20.984889	892.790790	12.321575
20.851567	883.711467	12.326579
20.886576	900.565065	12.331584
20.870519	880.680691	12.336589
20.586293	890.428997	12.341594
20.734928	888.495598	12.346599
20.643357	894.683964	12.351603
20.663946	894.122435	12.356608
20.828428	879.220820	12.361613
20.518460	889.935171	12.366618
20.761988	889.008501	12.371623
20.876024	890.419026	12.376627
20.725203	893.128625	12.381632
21.043415	888.247665	12.386637
20.808607	899.192886	12.391642
21.069109	903.223023	12.396647
20.973667	888.282431	12.401651
20.710819	893.859449	12.406656
20.850933	887.660180	12.411661
20.723588	891.608671	12.416666
20.923853	896.110461	12.421671
20.493782	893.707969	12.426675
20.575069	896.885173	12.431680
20.939561	894.273948	12.436685
20.746481	897.209485	12.441690
20.601293	895.065906	12.446695
20.826040	901.736832	12.451699
20.761554	893.881276	12.456704
20.643060	897.918245	12.461709
20.734216	902.092086	12.466714
20.825074	898.128902	12.471719
20.548349	900.193110	12.476723
20.640836	924.436630	12.481728
21.047602	925.259573	12.486733
20.963671	933.369044	12.491738
20.937796	914.864449	12.496743
20.985152	908.102800	12.501747
20.880461	910.857084	12.506752
20.947868	899.481230	12.511757
20.925688	898.691557	12.516762
20.757566	909.209833	12.521767
20.918442	909.587870	12.526771
20.775128	904.603898	12.531776
21.332856	901.238030	12.536781
20.871595	904.372461	12.541786
20.973047	907.671030	12.546791
20.765860	916.030386	12.551795
20.615900	910.072915	12.556800
20.635193	907.794290	12.561805
20.738057	905.272101	12.566810
20.808576	905.133116	12.571815
20.692388	906.902061	12.576819
20.487703	902.881935	12.581824
21.038238	900.595850	12.586829
20.901165	910.696014	12.591834
20.897353	904.160147	12.596839
20.999495	911.322142	12.601843
20.786933	908.192673	12.606848
21.300698	895.362641	12.611853
20.851275	900.193560	12.616858
21.035206	901.222354	12.621863
21.001499	908.081162	12.626867
20.626506	898.299207	12.631872
20.942846	896.255481	12.636877
20.742597	896.555497	12.641882
20.725106	892.341514	12.646887
20.815048	890.993064	12.651891
20.602084	889.700811	12.656896
20.795860	907.714962	12.661901
20.775164	910.810663	12.666906
20.818123	900.894236	12.671911
21.064212	912.040308	12.676915
20.682748	891.203374	12.681920
20.807489	889.890373	12.686925
20.539444	907.024128	12.691930
20.870534	907.170011	12.696935
20.896806	909.040814	12.701939
20.847582	916.097643	12.706944
20.824432	905.732863	12.711949
20.726088	898.871455	12.716954
21.124402	903.910938	12.721959
20.754229	888.053801	12.726963
20.417066	892.119337	12.731968
20.694836	885.937536	12.736973
20.951915	908.650367	12.741978
20.392714	914.170582	12.746983
20.668747	910.619406	12.751987
20.906600	920.746509	12.756992
21.208546	908.609418	12.761997
21.031893	913.649147	12.767002
20.954012	892.959332	12.772007
20.668484	897.317831	12.777011
20.729368	886.009260	12.782016
20.834971	880.564549	12.787021
20.835379	882.359049	12.792026
20.564609	883.988644	12.797031
20.701190	888.049581	12.802035
20.788277	904.524294	12.807040
21.106437	913.219326	12.812045
20.736860	900.139097	12.817050
20.752795	882.089922	12.822055
20.726239	896.518524	12.827059
20.693981	891.365456	12.832064
20.789154	894.362249	12.837069
20.974909	906.125066	12.842074
20.956176	895.202924	12.847079
20.898794	892.534409	12.852083
20.467776	886.659622	12.857088
20.977444	875.126515	12.862093
20.978453	890.735004	12.867098
21.030394	880.706771	12.872103
21.053054	879.462093	12.877107
20.915195	884.618627	12.882112
20.788601	876.386635	12.887117
20.918217	887.319453	12.892122
20.749122	887.042067	12.897127
20.871420	888.203693	12.902131
20.490234	892.714643	12.907136
20.710653	888.765490	12.912141
20.835485	890.995884	12.917146
20.746801	886.674987	12.922151
20.748519	885.257030	12.927155
20.629008	890.834839	12.932160
21.056608	874.814204	12.937165
20.633740	895.853512	12.942170
20.883956	883.566997	12.947175
20.733647	896.544043	12.952179
20.719704	893.089585	12.957184
20.944672	894.517109	12.962189
20.988772	882.873750	12.967194
21.047515	896.896087	12.972199
21.073511	886.914566	12.977203
20.805113	898.447038	12.982208
20.910494	882.294862	12.987213
21.071861	885.610678	12.992218
21.018479	878.108174	12.997223
21.050266	880.213059	13.002227
21.023343	882.928126	13.007232
20.961447	872.374008	13.012237
20.676366	858.876640	13.017242
20.690334	857.305345	13.022247
20.846606	852.388725	13.027251
20.746453	855.629552	13.032256
21.093598	859.671089	13.037261
20.830670	865.369534	13.042266
20.613419	858.301606	13.047271
20.812203	852.777389	13.052275
20.621571	864.273777	13.057280
20.969121	851.749414	13.062285
20.757204	855.004913	13.067290
20.640843	858.264095	13.072295
20.971108	859.660629	13.077299
20.686840	855.974907	13.082304
20.867760	855.430385	13.087309
20.306272	859.508037	13.092314
21.030614	871.177037	13.097319
21.056798	873.180313	13.102323
20.772419	867.208029	13.107328
20.946646	854.720770	13.112333
20.852567	863.481523	13.117338
20.645464	863.125046	13.122343
20.796576	861.118715	13.127347
20.488311	860.663255	13.132352
20.831679	856.931043	13.137357
20.625670	878.227472	13.142362
21.030545	880.689165	13.147367
20.739419	873.896363	13.152371
20.525115	867.272662	13.157376
20.968859	878.325681	13.162381
20.726068	882.961211	13.167386
20.788186	888.188352	13.172391
21.124807	890.996823	13.177395
20.871522	877.175823	13.182400
20.696031	871.865835	13.187405
20.700208	866.724312	13.192410
21.076905	864.025990	13.197415
21.045338	866.415367	13.202419
20.689568	863.091130	13.207424
20.781028	856.989519	13.212429
20.862166	878.796813	13.217434
20.900654	862.158589	13.222439
20.840225	861.652561	13.227443
20.892211	873.641690	13.232448
20.912624	862.304900	13.237453
20.836497	868.405635	13.242458
20.815759	871.565991	13.247463
20.900681	866.780594	13.252467
20.401242	861.506510	13.257472
21.064031	860.916669	13.262477
20.923322	866.709161	13.267482
20.734471	865.690608	13.272487
20.891321	864.807726	13.277491
20.321691	872.631933	13.282496
20.951972	859.947352	13.287501
20.661043	865.126716	13.292506
20.911569	867.094209	13.297511
21.129753	862.852106	13.302515
20.425121	875.225266	13.307520
21.000002	856.908776	13.312525
20.670845	866.022415	13.317530
20.538356	863.042610	13.322535
20.915073	862.768055	13.327539
20.757594	873.111143	13.332544
21.110943	853.029116	13.337549
20.752281	863.902601	13.342554
20.994583	863.606908	13.347559
21.172746	857.425236	13.352563
20.906770	868.968338	13.357568
21.026671	860.264955	13.362573
20.632896	860.535914	13.367578
20.743183	867.625625	13.372583
20.853312	870.047595	13.377587
20.728177	870.649444	13.382592
21.173578	863.240857	13.387597
20.834181	867.010276	13.392602
20.920535	863.736947	13.397607
21.051423	866.608189	13.402611
20.665676	860.849195	13.407616
21.205049	859.525258	13.412621
20.569781	852.689585	13.417626
20.555333	847.546308	13.422631
20.405264	854.026260	13.427635
20.370389	861.427703	13.432640
20.874793	871.367178	13.437645
20.791381	872.555305	13.442650
20.714303	875.190061	13.447655
20.748240	870.354448	13.452659
20.503718	882.521764	13.457664
20.995420	873.670763	13.462669
20.636032	878.282310	13.467674
20.624674	880.726813	13.472679
20.782042	886.419731	13.477683
20.801236	878.156600	13.482688
20.915091	874.932497	13.487693
20.597074	881.890256	13.492698
20.855132	876.127918	13.497703
21.079335	877.487754	13.502707
20.846170	881.035230	13.507712
20.828331	877.349585	13.512717
21.109663	881.721746	13.517722
20.580399	872.555771	13.522727
20.738697	881.747790	13.527731
20.627347	878.640030	13.532736
20.960405	875.805165	13.537741
20.564294	886.977953	13.542746
20.549767	885.635127	13.547751
20.567507	878.346783	13.552755
20.494622	895.487243	13.557760
20.749309	876.427015	13.562765
20.495571	879.244490	13.567770
20.978116	870.770265	13.572775
20.753634	888.155668	13.577779
20.771073	885.005289	13.582784
21.081143	888.779935	13.587789
20.886343	886.958083	13.592794
20.764073	884.446575	13.597799
21.017494	879.574375	13.602803
20.612378	885.984634	13.607808
20.998601	877.443767	13.612813
20.781444	903.360897	13.617818
21.405808	881.239183	13.622823
20.918427	882.233123	13.627827
20.764080	882.923210	13.632832
21.124113	883.387751	13.637837
21.041483	888.298935	13.642842
20.845199	894.861970	13.647847
21.079296	884.913490	13.652851
20.812796	872.709399	13.657856
20.967387	862.980196	13.662861
20.540818	865.087223	13.667866
20.757503	861.886145	13.672871
20.588753	863.542044	13.677875
20.545503	876.270184	13.682880
20.913807	876.473210	13.687885
20.590998	895.599488	13.692890
20.826848	886.675746	13.697895
20.930617	882.783047	13.702899
20.496693	883.763730	13.707904
20.775197	896.101525	13.712909
21.107388	885.990742	13.717914
21.156861	891.972106	13.722919
21.060428	876.079207	13.727923
20.695550	869.377019	13.732928
20.812336	860.484899	13.737933
20.679126	853.688997	13.742938
20.610209	863.590601	13.747943
20.677783	876.501338	13.752947
20.952662	877.152926	13.757952
20.811418	883.757639	13.762957
20.586173	901.072217	13.767962
20.948009	904.939535	13.772967
21.024385	888.564897	13.777971
20.657324	877.807136	13.782976
20.454631	860.951915	13.787981
20.700646	880.797999	13.792986
20.821936	888.393743	13.797991
21.283645	888.179749	13.802995
20.701502	872.015817	13.808000
20.757857	854.073770	13.813005
20.744745	870.219075	13.818010
20.959141	875.395115	13.823015
20.953753	858.978358	13.828019
20.601844	859.619530	13.833024
20.471609	855.679006	13.838029
20.787946	878.177334	13.843034
21.176314	879.883147	13.848039
20.943914	866.320599	13.853043
20.619706	858.118559	13.858048
20.838454	855.475394	13.863053
20.514655	866.286551	13.868058
20.695990	884.745780	13.873063
20.998296	876.970503	13.878067
20.682821	882.530679	13.883072
20.985904	882.168521	13.888077
20.610641	878.930968	13.893082
20.348780	874.424807	13.898087
20.585156	890.468840	13.903091
20.765171	888.842672	13.908096
21.054767	891.735915	13.913101
20.724038	904.457893	13.918106
20.880778	897.606263	13.923111
21.266481	888.625502	13.928115
20.700707	894.287107	13.933120
20.802817	885.545546	13.938125
20.497982	883.574088	13.943130
20.612527	900.164265	13.948135
20.598128	897.400584	13.953139
20.636396	897.045969	13.958144
21.273281	897.669781	13.963149
20.737123	905.083390	13.968154
20.909794	898.632918	13.973159
21.003269	900.521386	13.978163
20.771336	897.294084	13.983168
21.054255	880.856549	13.988173
21.054001	884.882540	13.993178
20.942025	865.544917	13.998183
20.630525	873.671729	14.003187
20.689901	862.194683	14.008192
20.650584	869.416362	14.013210
20.716681	873.256339	14.018227
20.403127	875.887518	14.023245
20.758224	887.333694	14.028263
20.901216	893.380813	14.033280
21.033462	894.904332	14.038298
21.109716	902.936125	14.043315
21.124503	907.416613	14.048333
21.219652	886.819656	14.053351
20.633327	885.403159	14.058368
21.029459	876.287776	14.063386
20.967435	874.760915	14.068403
20.958798	870.672680	14.073421
21.025122	877.840934	14.078439
20.799492	897.787039	14.083456
21.002889	893.086141	14.088474
21.091308	909.612961	14.093491
20.993558	912.038277	14.098509
21.161627	909.463318	14.103527
20.977635	914.052586	14.108544
21.124475	906.927380	14.113562
21.225308	907.092180	14.118579
21.150641	903.915756	14.123597
21.259612	908.884559	14.128615
20.776794	913.411384	14.133632
21.097906	913.934283	14.138650
20.917568	919.106527	14.143667
21.106172	902.551233	14.148685
21.225100	910.791715	14.153703
21.183323	910.408287	14.158720
21.325813	908.650614	14.163738
21.235055	911.496360	14.168755
20.939620	911.150245	14.173773
21.329511	916.387258	14.178791
21.137685	948.755776	14.183808
21.511888	947.167195	14.188826
21.481992	945.915184	14.193843
21.479643	944.537664	14.198861
21.665119	946.186398	14.203879
21.300590	951.394323	14.208896
21.372763	941.133567	14.213914
21.564440	938.281148	14.218931
21.249016	948.638889	14.223949
21.369941	933.047554	14.228967
21.772467	935.051754	14.233984
21.533606	948.120032	14.239002
21.363128	939.576300	14.244019
21.398280	937.676877	14.249037
21.722552	932.190669	14.254055
21.476807	949.568309	14.259072
21.590523	936.332803	14.264090
21.846963	939.384284	14.269107
21.705889	940.139768	14.274125
21.646631	922.183178	14.279143
21.668605	941.474835	14.284160
21.808188	934.330325	14.289178
21.744739	932.514266	14.294195
21.879352	937.796721	14.299213
22.100032	933.837051	14.304231
21.688257	946.986386	14.309248
21.765166	935.669440	14.314266
21.747101	932.402189	14.319283
21.554383	935.526882	14.324301
21.654225	942.088961	14.329319
21.798892	961.508932	14.334336
21.866958	968.486627	14.339354
22.192060	971.535029	14.344371
21.907456	973.132907	14.349389
22.404445	976.432304	14.354407
22.121536	976.685051	14.359424
22.366592	966.390411	14.364442
22.534921	947.513499	14.369459
22.121152	948.995131	14.374477
22.157373	944.253244	14.379495
22.189583	948.035728	14.384512
22.218126	934.120145	14.389530
22.021922	943.747902	14.394547
22.050322	938.617177	14.399565
22.411964	931.585106	14.404583
22.048862	934.628443	14.409600
22.144327	936.807454	14.414618
22.494144	928.111534	14.419635
21.861014	933.961582	14.424653
22.228216	942.983555	14.429671
22.839630	961.390039	14.434688
22.652329	942.840400	14.439706
22.494844	940.309497	14.444723
22.250517	938.402743	14.449741
22.420788	932.494384	14.454759
22.200607	947.853018	14.459776
22.316693	938.371727	14.464794
22.789101	933.632628	14.469811
22.525154	947.989993	14.474829
22.437779	929.798792	14.479847
22.318710	951.061821	14.484864
22.293597	941.340370	14.489882
22.753961	971.983223	14.494899
22.739006	965.229840	14.499917
23.001614	939.357212	14.504935
22.519527	955.006150	14.509952
22.427665	943.612302	14.514970
22.712886	940.999778	14.519987
22.538366	959.383758	14.525005
22.746815	960.495604	14.530023
22.784582	963.201318	14.535040
22.878644	965.059678	14.540058
22.833670	956.057070	14.545075
22.704345	946.352236	14.550093
22.588066	937.686610	14.555111
22.789613	955.375138	14.560128
22.982661	971.254593	14.565146
23.073088	962.710131	14.570163
22.503677	962.579162	14.575181
22.509068	964.160671	14.580199
22.959844	975.064723	14.585216
22.957511	974.887349	14.590234
23.169996	966.213311	14.595251
23.018912	979.684445	14.600269
23.367132	978.306060	14.605287
22.954200	976.069136	14.610304
22.893258	975.349009	14.615322
23.231814	970.255315	14.620339
22.514919	968.390899	14.625357
23.036459	978.553824	14.630375
22.910657	975.748889	14.635392
23.080361	968.251938	14.640410
23.329146	969.443863	14.645427
22.969775	969.277821	14.650445
23.358583	963.924444	14.655463
23.164258	971.927077	14.660480
23.003386	964.736098	14.665498
23.395168	968.340120	14.670515
23.211590	964.954551	14.675533
23.203736	963.351404	14.680551
23.311474	968.966902	14.685568
23.404009	968.244317	14.690586
23.563557	967.569242	14.695603
23.329714	971.804704	14.700621
23.553782	963.940455	14.705639
23.538717	962.247229	14.710656
23.550757	962.322378	14.715674
23.712113	961.356022	14.720691
23.495597	956.471981	14.725709
23.533821	956.039615	14.730727
23.845918	961.663411	14.735744
23.237803	961.423791	14.740762
23.532674	963.773910	14.745779
23.294855	967.914056	14.750797
23.746875	958.578934	14.755815
23.743836	963.142502	14.760832
23.501624	970.267209	14.765850
23.665702	959.057457	14.770867
23.404851	957.707010	14.775885
23.183409	967.631375	14.780903
23.498122	971.738447	14.785920
23.370942	971.021020	14.790938
23.273907	965.016863	14.795955
23.248750	989.629482	14.800973
23.824216	986.629329	14.805991
23.589421	991.083586	14.811008
23.450949	996.459954	14.816026
24.020277	999.088757	14.821043
23.941399	999.842188	14.826061
24.012635	1002.018782	14.831079
23.768315	1001.321610	14.836096
23.505649	997.824385	14.841114
24.078797	990.994492	14.846131
23.670105	1003.135132	14.851149
23.953484	992.302708	14.856167
23.864304	1002.545755	14.861184
23.654102	1012.572172	14.866202
23.943045	1007.996011	14.871219
24.317194	1022.410542	14.876237
24.406134	1024.688130	14.881255
24.305888	1003.966450	14.886272
24.294917	1004.638269	14.891290
24.289253	986.253076	14.896307
24.184803	998.826506	14.901325
24.262793	990.770049	14.906343
24.178869	983.258491	14.911360
24.063439	1001.452212	14.916378
24.291968	988.055209	14.921395
24.088301	994.299226	14.926413
24.182601	999.470164	14.931431
24.245139	1014.824672	14.936448
24.463015	1013.896487	14.941466
24.416913	1020.063476	14.946483
24.546846	1027.545685	14.951501
24.506776	1016.006674	14.956519
24.607052	1012.124385	14.961536
24.667631	996.177684	14.966554
24.630493	982.645316	14.971571
24.279397	978.501566	14.976589
24.468956	987.432357	14.981607
24.768118	980.838068	14.986624
24.689597	983.497842	14.991642
24.643950	981.633322	14.996659
24.574622	989.947919	15.001677
24.537151	979.366441	15.006695
24.892754	982.719850	15.011712
24.727620	990.549533	15.016730
25.103589	989.972066	15.021747
24.682772	984.985328	15.026765
24.692249	990.168218	15.031783
24.643014	985.172548	15.036800
24.502387	979.125005	15.041818
24.918714	981.040500	15.046835
24.569922	1000.331600	15.051853
25.070221	1001.077594	15.056871
25.197539	990.491846	15.061888
24.871323	998.830118	15.066906
24.730607	989.246616	15.071923
25.015045	989.050242	15.076941
24.939871	984.190837	15.081959
24.609704	997.292596	15.086976
24.858109	1013.751548	15.091994
25.208056	1014.659942	15.097011
25.191589	1019.986973	15.102029
24.957805	1014.338071	15.107047
25.015318	1012.828307	15.112064
25.084773	1027.494351	15.117082
25.250677	1014.745927	15.122099
25.143679	1015.267902	15.127117
25.273059	1017.468256	15.132135
25.089264	1008.287994	15.137152
24.774718	1016.078603	15.142170
25.412465	1004.396887	15.147187
25.207036	1023.098893	15.152205
24.947734	1020.620392	15.157223
25.133856	1013.954460	15.162240
24.994081	1020.078191	15.167258
25.147379	1009.293241	15.172275
25.052075	1010.456685	15.177293
25.279619	1010.791602	15.182311
25.168044	1017.025660	15.187328
25.378007	1035.431778	15.192346
25.828540	1035.704391	15.197363
25.564526	1037.914012	15.202381
25.469544	1032.469469	15.207399
25.648049	1023.882609	15.212416
25.539579	1016.843686	15.217434
25.557112	1006.148029	15.222451
25.708446	1022.817519	15.227469
25.589270	1024.656417	15.232487
25.646488	1023.594988	15.237504
25.536460	1028.707295	15.242522
25.761246	1033.223537	15.247539
25.615007	1045.468636	15.252557
25.645370	1047.156278	15.257575
26.057411	1040.883714	15.262592
26.113343	1033.203540	15.267610
25.831000	1014.228544	15.272627
25.668035	1017.546699	15.277645
25.404779	1016.162025	15.282663
26.073327	1022.683769	15.287680
25.937764	1035.888225	15.292698
25.854447	1028.678552	15.297715
25.938895	1037.764558	15.302733
25.835083	1035.906162	15.307751
26.233924	1030.052538	15.312768
26.412216	1027.908488	15.317786
26.260867	1023.416704	15.322803
25.849563	1018.698983	15.327821
25.976257	1026.194291	15.332839
26.330548	1033.988340	15.337856
25.959960	1028.774936	15.342874
26.230681	1031.007802	15.347891
26.289292	1036.403085	15.352909
25.946871	1042.364102	15.357927
26.416163	1041.142571	15.362944
26.366271	1031.022337	15.367962
26.316921	1027.423444	15.372979
26.220182	1040.550930	15.377997
26.208532	1036.131237	15.383015
26.507789	1030.622241	15.388032
26.281319	1035.918282	15.393050
26.335461	1027.277328	15.398067
26.404405	1035.376425	15.403085
25.954238	1045.480461	15.408103
26.417863	1040.605882	15.413120
26.235935	1039.609335	15.418138
26.174405	1039.778012	15.423155
26.174475	1033.511387	15.428173
26.317844	1037.773215	15.433191
26.438517	1029.914412	15.438208
26.193491	1029.055337	15.443226
26.246275	1035.936408	15.448243
26.776574	1053.659135	15.453261
26.869272	1057.587722	15.458279
26.864937	1044.532959	15.463296
26.473874	1033.620894	15.468314
27.175557	1043.799177	15.473331
26.813749	1037.517912	15.478349
26.734926	1046.752655	15.483367
26.620760	1027.536897	15.488384
26.343922	1044.279422	15.493402
26.670597	1035.170300	15.498419
26.826747	1067.799746	15.503437
27.005918	1063.101084	15.508455
27.216283	1055.201221	15.513472
27.012116	1054.853128	15.518490
27.087423	1056.983465	15.523507
27.172823	1064.626945	15.528525
27.236283	1046.765452	15.533543
27.491392	1023.700004	15.538560
26.968626	1028.749159	15.543578
26.934378	1026.745969	15.548595
27.038267	1032.078975	15.553613
27.029703	1020.534935	15.558631
27.324910	1010.150472	15.563648
27.012943	1032.385007	15.568666
27.019473	1031.017073	15.573683
26.966819	1047.110397	15.578701
27.243972	1059.185737	15.583719
27.626489	1064.608016	15.588736
27.551950	1060.008020	15.593754
27.174801	1045.147204	15.598771
27.463942	1058.641001	15.603789
27.228622	1074.894044	15.608807
27.632695	1058.672276	15.613824
27.825583	1065.015088	15.618842
27.411094	1039.412288	15.623859
27.699822	1024.157441	15.628877
27.198044	1032.898094	15.633895
27.577183	1018.961115	15.638912
27.493668	1029.184403	15.643930
27.410499	1036.436351	15.648947
27.429462	1054.172998	15.653965
27.411331	1059.572664	15.658983
27.578105	1062.644766	15.664000
27.277018	1053.704967	15.669018
27.431195	1058.727957	15.674035
27.645744	1064.071638	15.679053
27.701040	1063.476105	15.684071
27.852218	1051.013128	15.689088
27.842835	1059.068105	15.694106
27.784444	1059.376274	15.699123
28.173370	1035.507709	15.704141
27.910108	1065.946871	15.709159
27.752864	1060.592467	15.714176
27.673041	1056.655525	15.719194
27.936394	1066.386236	15.724211
27.741907	1058.712957	15.729229
27.735019	1056.868985	15.734247
27.997818	1057.648144	15.739264
27.920391	1061.095804	15.744282
27.613598	1071.815607	15.749299
27.864743	1076.788533	15.754317
28.106119	1080.652516	15.759335
28.555674	1088.541507	15.764352
28.333392	1072.798704	15.769370
28.330863	1071.694894	15.774387
28.462296	1052.430493	15.779405
28.162600	1058.515257	15.784423
28.260325	1056.053734	15.789440
28.282135	1052.342817	15.794458
28.112843	1053.003711	15.799475
28.215942	1053.415105	15.804493
28.163350	1059.622470	15.809511
28.596506	1064.207730	15.814528
28.373153	1064.775005	15.819546
28.493620	1069.469911	15.824563
28.418989	1061.337088	15.829581
28.351099	1078.485179	15.834599
28.666647	1067.883510	15.839616
28.701397	1066.596011	15.844634
28.392353	1081.948512	15.849651
28.498148	1077.050773	15.854669
28.751121	1075.585330	15.859687
28.813325	1080.434243	15.864704
28.541621	1085.720214	15.869722
28.770071	1076.124962	15.874739
28.810171	1078.971890	15.879757
28.409009	1079.680778	15.884775
28.751521	1068.613934	15.889792
28.809463	1072.577955	15.894810
28.797033	1081.578772	15.899827
28.929432	1081.658320	15.904845
28.749860	1095.445548	15.909863
29.092707	1078.978705	15.914880
28.875674	1085.879239	15.919898
29.038198	1074.586280	15.924915
28.818613	1089.026366	15.929933
28.997967	1080.382712	15.934951
28.784333	1076.015670	15.939968
28.913005	1074.398601	15.944986
28.826132	1068.902415	15.950003
28.921478	1082.285579	15.955021
28.851196	1078.578333	15.960039
28.818261	1064.795119	15.965056
28.665817	1074.197343	15.970074
28.888383	1099.220502	15.975091
29.632245	1099.364539	15.980109
29.386277	1103.595680	15.985127
29.252464	1085.992107	15.990144
29.491261	1076.632720	15.995162
29.057523	1074.067206	16.000179
29.106378	1090.575376	16.005197
29.530198	1100.742964	16.010215
29.267967	1096.569276	16.015232
29.377692	1100.405501	16.020250
29.308387	1102.562056	16.025267
29.422011	1088.252100	16.030285
29.403714	1106.141037	16.035303
29.468068	1089.374124	16.040320
29.671655	1095.422674	16.045338
29.420905	1093.435130	16.050355
29.468151	1100.142517	16.055373
29.517232	1101.619550	16.060391
29.459023	1102.874607	16.065408
29.679093	1096.187493	16.070426
29.446333	1104.885282	16.075443
29.834762	1090.345886	16.080461
29.341855	1101.543686	16.085479
29.779555	1095.578451	16.090496
30.052875	1097.557668	16.095514
29.890235	1107.719703	16.100531
30.108113	1098.234656	16.105549
29.802356	1089.018740	16.110567
29.637520	1084.148434	16.115584
29.925302	1111.948480	16.120602
29.735981	1112.354606	16.125619
30.679541	1129.385480	16.130637
30.431174	1127.457323	16.135655
30.220588	1105.003971	16.140672
30.517637	1086.943158	16.145690
30.149487	1101.271679	16.150707
30.382207	1099.897548	16.155725
30.353272	1087.395630	16.160743
30.125098	1107.502871	16.165760
30.279644	1099.731431	16.170778
30.251562	1094.505844	16.175795
30.343832	1094.192263	16.180813
30.135245	1093.188953	16.185831
29.986933	1098.776130	16.190848
30.614238	1099.283233	16.195866
30.231358	1088.195223	16.200883
30.369315	1111.679397	16.205901
30.494285	1089.970037	16.210919
30.033421	1116.259919	16.215936
30.430501	1104.526850	16.220954
30.154547	1137.053919	16.225971
30.734407	1110.307731	16.230989
30.205897	1149.741046	16.236007
30.684825	1131.495447	16.241024
30.571382	1125.865058	16.246042
30.797068	1137.597904	16.251059
30.965084	1126.554128	16.256077
31.009808	1128.516329	16.261095
30.790777	1137.215093	16.266112
30.912480	1125.354477	16.271130
30.659502	1126.739696	16.276147
31.154582	1107.278803	16.281165
30.577964	1130.252515	16.286183
30.949662	1121.483782	16.291200
30.919821	1109.131420	16.296218
30.960176	1144.639135	16.301235
30.897381	1123.466164	16.306253
30.751105	1134.534775	16.311271
30.732750	1136.601415	16.316288
31.048120	1138.517305	16.321306
31.004464	1147.096872	16.326323
30.991895	1117.141953	16.331341
31.084602	1136.973123	16.336359
31.021921	1140.107005	16.341376
30.872690	1114.038641	16.346394
30.766186	1149.300816	16.351411
31.076482	1128.305848	16.356429
30.971600	1148.870087	16.361447
31.587491	1154.437642	16.366464
31.511183	1142.723418	16.371482
31.278202	1173.782439	16.376499
31.749255	1144.219071	16.381517
31.388525	1157.091478	16.386535
31.217739	1133.082372	16.391552
31.533363	1143.183881	16.396570
31.571998	1147.026738	16.401587
31.901219	1149.991156	16.406605
31.617089	1145.943636	16.411623
31.486246	1132.404052	16.416640
31.781534	1106.000547	16.421658
31.478600	1123.099666	16.426675
31.729140	1119.209113	16.431693
31.750553	1136.906146	16.436711
31.529260	1133.120729	16.441728
31.788119	1142.328415	16.446746
31.866678	1133.416101	16.451763
32.001061	1145.182391	16.456781
31.972271	1155.716350	16.461799
31.854075	1159.732081	16.466816
32.153958	1144.727002	16.471834
31.825422	1138.195005	16.476851
32.251863	1143.180892	16.481869
32.216956	1128.710550	16.486887
32.008533	1126.231780	16.491904
31.899808	1111.002482	16.496922
32.055789	1123.090910	16.501939
32.085345	1113.763299	16.506957
32.039631	1127.908291	16.511975
31.925697	1140.154609	16.516992
32.273277	1133.664209	16.522010
32.001126	1145.736001	16.527027
32.031963	1151.602924	16.532045
32.324281	1152.956229	16.537063
32.353130	1147.147414	16.542080
32.303965	1154.280744	16.547098
32.309193	1142.646321	16.552115
32.471491	1143.941714	16.557133
32.301763	1164.838774	16.562151
32.253288	1153.790182	16.567168
32.693614	1142.636899	16.572186
31.985263	1152.225360	16.577203
32.069056	1147.622104	16.582221
32.561188	1150.996248	16.587239
32.448568	1149.011832	16.592256
32.531446	1142.123218	16.597274
32.443343	1150.727179	16.602291
32.488184	1148.838767	16.607309
32.303155	1153.752304	16.612327
32.389807	1170.520367	16.617344
32.669281	1165.632649	16.622362
32.632539	1171.077795	16.627379
32.807764	1174.818654	16.632397
32.841534	1167.675176	16.637415
32.967478	1173.869845	16.642432
33.323462	1166.888899	16.647450
32.993059	1158.284031	16.652467
33.113160	1152.525151	16.657485
33.234289	1162.343103	16.662503
33.033239	1158.482095	16.667520
33.598558	1140.321802	16.672538
33.327407	1159.441861	16.677555
33.402584	1148.310634	16.682573
33.679798	1154.194890	16.687591
33.272074	1141.567730	16.692608
33.129963	1132.858917	16.697626
33.553133	1130.567262	16.702643
33.456537	1126.334115	16.707661
33.417517	1130.335638	16.712679
33.150719	1141.637398	16.717696
33.299021	1128.644727	16.722714
33.114581	1131.439393	16.727731
33.365154	1140.967710	16.732749
33.541560	1147.816534	16.737767
33.366755	1148.251805	16.742784
33.764608	1143.930354	16.747802
33.675971	1144.773435	16.752819
33.690968	1150.161560	16.757837
33.801783	1143.784419	16.762855
33.334767	1142.658735	16.767872
33.654110	1145.909432	16.772890
33.489115	1153.512675	16.777907
33.560610	1155.303877	16.782925
33.965794	1154.562877	16.787943
33.642359	1146.414635	16.792960
33.724319	1142.141994	16.797978
33.436632	1147.148977	16.802995
33.699093	1155.802417	16.808013
33.885007	1159.261580	16.813031
33.688772	1152.997899	16.818048
33.982335	1156.142604	16.823066
33.711015	1143.695025	16.828083
33.629369	1146.185448	16.833101
33.703397	1166.170642	16.838119
33.716030	1175.140780	16.843136
34.011119	1168.628850	16.848154
34.048342	1183.180648	16.853171
33.981924	1182.182970	16.858189
34.065906	1174.847444	16.863207
34.104888	1179.390221	16.868224
34.359977	1172.286944	16.873242
34.209238	1183.991780	16.878259
34.453548	1176.084865	16.883277
34.206335	1169.948852	16.888295
34.368923	1176.928876	16.893312
34.355444	1172.830317	16.898330
34.370307	1173.524763	16.903347
34.259190	1191.293335	16.908365
34.893463	1194.737624	16.913383
34.538754	1199.697114	16.918400
34.967952	1189.505077	16.923418
34.543799	1183.403570	16.928435
34.432453	1184.382404	16.933453
34.724368	1190.026813	16.938471
34.632671	1206.521354	16.943488
35.059611	1208.318790	16.948506
35.051091	1206.498654	16.953523
34.997593	1190.820034	16.958541
34.759687	1171.804709	16.963559
34.880034	1181.586621	16.968576
34.924366	1164.560129	16.973594
34.878310	1173.100770	16.978611
34.928477	1193.744159	16.983629
35.301720	1196.117997	16.988647
35.219168	1198.756432	16.993664
34.885872	1173.719293	16.998682
34.954712	1180.759887	17.003699
35.125020	1191.954220	17.008717
35.464552	1191.550866	17.013735
35.324679	1191.686423	17.018752
35.440426	1190.079268	17.023770
35.395097	1184.054189	17.028787
35.231640	1181.980353	17.033805
35.113534	1174.840646	17.038823
35.128943	1188.172166	17.043840
35.083678	1200.410729	17.048858
35.054787	1200.080292	17.053875
35.308375	1192.805792	17.058893
35.682949	1187.045636	17.063911
35.316023	1199.497515	17.068928
35.530113	1195.765332	17.073946
35.654045	1187.876037	17.078963
35.042601	1195.042440	17.083981
35.445223	1195.742680	17.088999
35.622122	1194.504855	17.094016
35.742270	1194.798707	17.099034
35.720978	1197.642867	17.104051
35.559927	1212.729666	17.109069
36.056796	1219.963124	17.114087
35.886487	1224.597495	17.119104
36.202759	1211.702224	17.124122
36.007827	1191.218737	17.129139
35.907867	1195.752221	17.134157
36.002214	1180.057896	17.139175
35.925764	1190.585326	17.144192
36.073464	1209.110132	17.149210
36.210306	1214.710074	17.154227
36.203254	1218.009699	17.159245
36.330101	1191.016303	17.164263
36.178012	1188.852567	17.169280
36.257034	1193.930061	17.174298
36.350051	1181.474675	17.179315
36.374817	1192.869967	17.184333
36.149545	1188.981354	17.189351
36.468905	1197.111386	17.194368
36.267932	1184.558174	17.199386
36.440871	1208.905201	17.204403
36.379091	1219.238410	17.209421
36.662414	1208.531671	17.214439
36.341037	1221.734473	17.219456
36.214349	1216.579623	17.224474
36.734154	1215.993366	17.229491
36.751109	1225.758765	17.234509
36.732019	1217.922151	17.239527
36.738530	1225.152025	17.244544
36.813327	1223.167594	17.249562
36.734778	1212.394304	17.254579
36.915679	1223.456416	17.259597
36.783654	1215.370412	17.264615
36.574777	1225.807307	17.269632
36.609922	1214.133449	17.274650
37.144371	1214.617618	17.279667
36.911018	1215.625350	17.284685
36.740814	1220.099261	17.289703
36.670789	1218.443083	17.294720
36.676888	1216.505787	17.299738
36.820441	1224.179401	17.304755
36.768981	1223.770769	17.309773
37.226298	1223.617605	17.314791
37.111028	1236.656992	17.319808
37.263731	1246.380307	17.324826
37.642710	1236.400732	17.329843
37.658730	1248.807306	17.334861
37.334236	1231.232395	17.339879
37.116524	1217.110432	17.344896
37.505693	1222.291048	17.349914
37.391806	1224.667082	17.354931
36.950437	1240.967330	17.359949
37.237751	1245.023799	17.364967
37.484433	1242.099630	17.369984
37.514145	1250.897211	17.375002
37.600902	1244.256459	17.380019
37.340941	1251.305485	17.385037
37.822445	1240.213197	17.390055
37.421347	1253.022917	17.395072
37.587582	1244.689559	17.400090
37.420873	1237.746329	17.405107
37.476639	1237.668220	17.410125
37.765769	1236.527318	17.415143
37.991440	1265.438643	17.420160
37.814130	1258.644952	17.425178
38.117856	1247.629775	17.430195
38.272203	1256.086595	17.435213
38.286187	1245.874228	17.440231
38.096491	1249.276920	17.445248
37.821962	1236.781010	17.450266
37.837794	1242.129713	17.455283
38.204100	1268.490857	17.460301
38.683568	1254.366198	17.465319
38.231983	1240.849354	17.470336
38.376800	1231.921692	17.475354
38.319880	1232.441980	17.480371
38.201233	1232.237538	17.485389
38.171103	1226.438097	17.490407
38.287446	1243.516103	17.495424
38.889916	1252.335589	17.500442
38.542934	1252.916296	17.505459
38.551489	1249.706073	17.510477
38.976583	1244.526127	17.515495
38.670157	1233.844219	17.520512
38.249174	1230.265223	17.525530
38.537871	1228.558123	17.530547
38.825487	1244.402350	17.535565
38.878537	1259.458196	17.540583
39.047007	1251.413904	17.545600
38.695256	1238.411229	17.550618
39.146243	1228.273890	17.555635
38.760093	1219.652707	17.560653
39.010625	1204.779701	17.565671
38.751440	1221.665900	17.570688
38.912219	1231.394209	17.575706
39.388155	1232.417800	17.580723
39.010905	1216.432151	17.585741
38.939324	1219.580053	17.590759
39.047003	1232.649943	17.595776
39.107069	1243.194962	17.600794
39.214572	1255.306963	17.605811
38.851957	1263.660628	17.610829
39.399383	1251.840544	17.615847
39.322128	1253.793904	17.620864
39.084720	1243.804097	17.625882
39.368878	1244.081230	17.630899
39.526627	1258.401531	17.635917
39.579155	1244.870346	17.640935
39.323475	1246.652395	17.645952
39.767447	1228.786615	17.650970
39.370593	1243.725445	17.655987
39.338751	1239.296326	17.661005
39.666177	1247.459706	17.666023
39.535727	1245.552050	17.671040
39.432597	1246.315653	17.676058
39.751560	1236.699567	17.681075
39.326925	1252.114726	17.686093
39.116066	1239.843030	17.691111
39.301662	1252.364129	17.696128
39.049045	1272.763351	17.701146
39.610524	1272.700536	17.706163
39.521110	1285.732698	17.711181
39.509519	1277.548801	17.716199
40.093191	1284.257233	17.721216
40.011683	1306.117242	17.726234
40.450543	1303.344875	17.731251
40.188842	1297.110448	17.736269
40.639660	1299.478223	17.741287
40.387807	1270.976823	17.746304
40.245706	1272.032923	17.751322
40.282119	1265.782423	17.756339
40.244380	1270.287130	17.761357
40.195668	1273.058603	17.766375
40.324476	1270.028963	17.771392
40.405773	1292.471725	17.776410
40.550177	1304.982137	17.781427
40.741474	1308.868327	17.786445
40.711981	1291.087422	17.791463
40.576704	1281.803294	17.796480
41.089908	1274.108262	17.801498
41.123413	1267.367457	17.806515
40.382547	1277.190838	17.811533
40.443735	1262.778964	17.816551
40.626439	1263.773824	17.821568
40.796107	1294.311151	17.826586
40.817346	1285.346539	17.831603
40.770936	1298.093437	17.836621
40.838570	1298.397240	17.841639
40.913972	1306.515908	17.846656
40.546893	1305.712460	17.851674
40.996406	1299.043714	17.856691
40.890574	1302.675280	17.861709
40.833622	1300.793646	17.866727
40.933275	1291.753604	17.871744
40.596874	1292.206788	17.876762
40.759737	1307.348986	17.881779
40.965993	1317.949392	17.886797
41.716088	1317.323257	17.891815
41.618113	1318.842643	17.896832
41.328211	1318.610458	17.901850
41.841518	1318.108603	17.906867
41.431583	1314.911629	17.911885
41.304245	1316.854109	17.916903
41.871793	1314.956239	17.921920
41.550791	1315.331464	17.926938
41.768564	1307.258829	17.931955
41.649348	1301.791307	17.936973
41.708810	1296.115971	17.941991
41.703416	1287.111563	17.947008
41.334791	1305.784907	17.952026
42.093289	1312.015599	17.957043
42.107456	1312.541855	17.962061
42.080344	1310.737254	17.967079
41.831611	1292.193816	17.972096
41.851721	1288.612093	17.977114
42.164245	1298.553764	17.982131
42.362064	1317.043976	17.987149
41.843661	1290.909905	17.992167
42.126022	1286.573800	17.997184
41.750192	1310.041144	18.002202
42.127440	1303.928170	18.007219
42.301630	1310.481706	18.012237
41.903211	1317.986987	18.017255
42.036830	1313.790998	18.022272
42.035216	1321.091427	18.027290
42.092402	1310.297988	18.032307
42.271969	1311.151783	18.037325
42.227553	1320.876700	18.042343
42.499602	1315.029030	18.047360
42.439264	1342.759206	18.052378
42.566775	1344.145107	18.057395
42.296012	1345.514306	18.062413
42.488827	1343.432387	18.067431
42.736622	1344.957975	18.072448
42.508543	1351.424682	18.077466
42.946793	1345.916996	18.082483
42.752177	1337.178681	18.087501
42.766172	1348.983215	18.092519
42.907018	1346.079051	18.097536
42.489554	1349.389109	18.102554
42.849338	1350.155964	18.107571
43.277371	1346.664892	18.112589
42.795190	1348.879468	18.117607
43.233525	1348.141038	18.122624
42.667270	1346.765330	18.127642
42.778460	1359.416362	18.132659
43.276719	1368.257259	18.137677
43.461513	1363.642546	18.142695
43.372193	1359.390866	18.147712
43.342232	1360.679192	18.152730
43.468256	1364.319412	18.157747
43.401714	1367.173968	18.162765
43.313160	1367.881771	18.167783
43.508815	1366.395556	18.172800
43.209696	1370.330878	18.177818
43.492388	1370.394323	18.182835
43.376863	1365.452351	18.187853
43.409283	1367.701256	18.192871
43.897904	1358.100503	18.197888
43.476561	1370.953666	18.202906
43.716589	1365.888921	18.207923
44.003432	1351.096488	18.212941
43.840160	1357.293319	18.217959
44.116051	1362.767326	18.222976
44.007709	1353.062016	18.227994
44.053351	1359.758769	18.233011
43.720350	1357.496449	18.238029
44.097324	1356.703314	18.243047
44.080512	1360.102053	18.248064
43.594038	1368.816868	18.253082
43.893507	1356.926138	18.258099
44.530811	1371.763867	18.263117
44.209349	1385.065928	18.268135
44.342743	1388.558691	18.273152
44.713470	1383.769603	18.278170
44.503958	1373.116178	18.283187
44.592005	1355.959009	18.288205
44.269775	1350.838442	18.293223
44.478430	1356.587430	18.298240
44.300036	1367.335734	18.303258
44.413746	1371.274426	18.308275
44.768950	1381.435857	18.313293
44.595640	1379.583781	18.318311
44.752084	1377.531252	18.323328
44.664604	1381.505968	18.328346
44.740389	1370.687496	18.333363
44.752715	1383.796325	18.338381
44.611772	1386.763422	18.343399
44.924537	1371.867736	18.348416
44.709263	1378.513304	18.353434
44.862189	1387.911072	18.358451
44.944293	1371.189763	18.363469
44.779023	1377.965779	18.368487
45.174798	1386.637422	18.373504
45.207793	1395.360637	18.378522
45.640342	1394.832335	18.383539
45.693030	1379.838124	18.388557
45.195966	1382.555286	18.393575
45.505392	1372.721988	18.398592
45.652066	1383.025214	18.403610
45.556575	1377.104006	18.408627
45.475905	1370.760452	18.413645
45.490401	1380.582976	18.418663
45.305941	1382.157059	18.423680
45.351285	1384.411771	18.428698
45.728630	1395.304263	18.433715
45.898178	1391.761601	18.438733
45.493417	1395.393676	18.443751
45.742386	1389.029000	18.448768
45.744185	1405.847048	18.453786
45.789116	1409.951660	18.458803
46.075721	1394.301944	18.463821
45.924516	1405.470645	18.468839
45.755181	1400.040966	18.473856
45.907187	1401.042304	18.478874
45.830993	1401.381633	18.483891
45.868381	1398.552160	18.488909
45.873283	1411.893427	18.493927
46.224245	1400.334213	18.498944
45.998399	1409.529716	18.503962
45.702832	1406.849296	18.508979
46.104019	1407.326414	18.513997
46.287055	1424.966564	18.519015
46.686558	1430.446049	18.524032
46.748085	1432.662009	18.529050
46.637740	1427.211901	18.534067
46.737064	1432.141526	18.539085
46.407396	1416.248737	18.544103
46.980043	1414.003986	18.549120
46.629635	1403.829174	18.554138
46.576742	1409.259683	18.559155
46.935479	1404.283742	18.564173
46.960411	1424.000279	18.569191
46.965982	1430.207964	18.574208
46.788161	1422.943954	18.579226
46.878675	1417.965170	18.584243
47.218884	1412.908813	18.589261
47.131749	1432.273582	18.594279
47.321941	1407.246926	18.599296
46.815483	1411.945978	18.604314
46.729252	1433.611882	18.609331
46.997709	1420.980450	18.614349
47.200197	1418.944167	18.619367
47.096965	1419.852510	18.624384
47.240231	1427.979299	18.629402
47.288803	1424.117731	18.634419
47.481992	1414.136207	18.639437
47.156210	1427.852690	18.644455
47.510096	1419.214033	18.649472
47.651136	1423.367812	18.654490
47.173480	1424.821924	18.659507
47.448578	1432.732640	18.664525
47.774663	1445.406102	18.669543
47.490832	1446.972446	18.674560
47.688045	1459.049862	18.679578
47.755059	1457.849989	18.684595
47.762522	1442.828320	18.689613
47.830256	1450.331681	18.694631
47.989917	1437.289733	18.699648
48.234736	1450.684005	18.704666
47.801174	1455.100892	18.709683
48.255097	1451.578926	18.714701
47.937710	1452.573335	18.719719
48.049327	1443.775104	18.724736
48.220645	1446.122990	18.729754
48.590058	1434.771587	18.734771
48.435256	1442.816938	18.739789
48.234582	1450.589616	18.744807
48.457361	1438.621390	18.749824
48.584893	1431.417212	18.754842
48.338643	1450.711430	18.759859
48.528123	1442.679412	18.764877
48.296458	1433.753470	18.769895
48.390089	1443.638919	18.774912
48.380202	1451.233309	18.779930
48.429911	1462.788426	18.784947
48.827779	1479.324747	18.789965
48.641261	1474.217097	18.794983
48.961180	1472.980034	18.800000
49.248931	1466.621723	18.805018
48.716959	1476.916850	18.810035
49.163821	1468.186258	18.815053
48.654520	1480.854561	18.820071
48.908387	1464.627984	18.825088
49.000624	1483.970507	18.830106
49.308393	1469.316186	18.835123
49.353509	1464.572710	18.840141
49.006553	1484.658519	18.845159
49.130588	1468.062543	18.850176
49.229880	1459.579294	18.855194
49.284500	1458.796667	18.860211
49.275562	1469.849921	18.865229
49.384153	1481.552962	18.870247
49.867660	1462.595227	18.875264
49.588605	1483.848375	18.880282
49.619393	1484.900512	18.885299
49.849876	1473.503598	18.890317
50.059421	1473.021871	18.895335
49.933712	1467.588355	18.900352
49.845879	1470.867888	18.905370
49.855772	1481.545350	18.910387
49.874159	1474.456083	18.915405
50.155354	1474.360896	18.920423
49.806010	1482.147864	18.925440
49.969659	1474.083770	18.930458
50.033051	1480.821792	18.935475
50.355148	1472.617599	18.940493
50.167120	1479.587624	18.945511
49.878129	1475.498313	18.950528
50.479745	1468.556700	18.955546
50.341692	1472.031429	18.960563
50.374947	1477.915403	18.965581
50.217347	1474.281754	18.970599
50.250131	1463.740626	18.975616
50.674933	1466.408303	18.980634
50.495964	1479.237848	18.985651
50.684358	1471.632268	18.990669
50.198237	1465.084354	18.995687
50.056157	1477.108935	19.000704
50.245660	1493.529069	19.005722
50.307869	1503.284293	19.010739
50.587746	1497.842707	19.015757
50.724481	1493.836501	19.020775
50.943587	1489.886371	19.025792
51.103204	1489.159355	19.030810
50.944296	1496.075981	19.035827
51.308753	1493.469600	19.040845
51.018168	1491.791939	19.045863
51.151536	1507.576114	19.050880
51.410127	1516.027474	19.055898
51.017291	1527.274129	19.060915
51.456287	1520.679319	19.065933
51.669627	1520.572932	19.070951
51.806803	1513.450544	19.075968
51.461191	1509.455196	19.080986
51.401231	1502.329647	19.086003
51.843862	1501.247614	19.091021
51.720585	1509.262806	19.096039
51.344515	1503.674153	19.101056
51.676254	1507.797543	19.106074
51.884241	1514.577013	19.111091
51.765555	1516.861052	19.116109
51.678047	1509.854723	19.121127
51.842777	1512.398722	19.126144
51.695725	1509.919534	19.131162
51.542663	1503.080962	19.136179
52.114515	1511.867742	19.141197
51.865633	1504.536373	19.146215
51.646908	1513.944734	19.151232
52.527257	1525.389448	19.156250
52.088514	1542.531168	19.161267
52.428939	1542.064745	19.166285
52.454098	1541.853092	19.171303
52.370280	1542.720594	19.176320
52.655267	1539.338808	19.181338
52.515153	1545.931568	19.186355
52.493072	1529.157481	19.191373
52.942020	1538.096010	19.196391
52.657813	1534.092434	19.201408
52.929132	1535.505755	19.206426
52.783344	1534.781828	19.211443
52.931801	1535.052297	19.216461
52.872818	1531.343132	19.221479
52.673062	1530.371413	19.226496
52.858628	1531.950991	19.231514
52.485515	1542.686434	19.236531
52.490531	1530.148831	19.241549
52.554483	1537.265883	19.246567
52.722542	1553.129517	19.251584
53.036929	1554.169463	19.256602
53.034501	1565.152539	19.261619
53.260963	1558.632506	19.266637
53.559709	1562.561404	19.271655
53.046703	1561.230661	19.276672
53.243619	1550.512285	19.281690
53.494784	1562.876908	19.286707
53.537880	1557.523399	19.291725
53.514756	1555.793636	19.296743
53.476531	1563.477546	19.301760
53.740961	1571.659024	19.306778
53.947109	1578.781732	19.311795
54.110762	1580.514246	19.316813
53.715652	1568.262217	19.321831
53.991422	1575.175621	19.326848
54.415316	1562.097712	19.331866
54.027938	1561.388718	19.336883
54.019978	1555.046070	19.341901
53.998379	1557.125871	19.346919
53.939818	1572.363436	19.351936
54.262414	1587.902019	19.356954
54.332509	1589.383617	19.361971
54.246287	1584.097913	19.366989
54.515800	1585.804106	19.372007
54.275779	1593.196176	19.377024
54.586010	1582.174991	19.382042
54.458245	1590.865761	19.387059
54.397982	1584.199539	19.392077
54.562325	1589.782657	19.397095
54.332384	1585.573786	19.402112
54.410335	1572.705194	19.407130
54.545217	1598.443191	19.412147
54.877916	1585.209921	19.417165
54.590021	1589.237105	19.422183
54.825514	1606.988660	19.427200
55.318152	1602.382977	19.432218
54.938675	1617.854239	19.437235
55.170793	1608.890401	19.442253
55.011707	1608.725434	19.447271
55.084644	1612.021831	19.452288
55.279390	1608.269034	19.457306
55.639012	1619.128344	19.462323
55.535878	1605.187499	19.467341
55.204673	1609.951470	19.472359
55.258210	1623.057089	19.477376
55.301737	1601.136585	19.482394
55.277785	1608.006572	19.487411
55.295595	1610.361664	19.492429
55.481643	1618.561961	19.497447
55.766691	1638.356854	19.502464
55.910105	1638.928575	19.507482
56.284632	1639.449280	19.512499
56.087297	1623.782119	19.517517
56.079702	1614.438088	19.522535
55.541209	1602.740572	19.527552
56.037271	1610.090763	19.532570
56.143248	1624.537660	19.537587
56.024579	1632.910830	19.542605
56.356192	1629.899110	19.547623
56.178904	1631.601061	19.552640
56.183488	1630.735171	19.557658
56.413029	1630.577437	19.562675
56.122103	1623.277881	19.567693
56.433039	1630.781874	19.572711
56.196221	1628.417654	19.577728
56.451231	1626.396562	19.582746
56.481493	1631.920857	19.587763
56.465825	1634.808250	19.592781
56.529156	1615.934631	19.597799
56.406646	1626.455565	19.602816
57.094942	1637.578646	19.607834
56.714474	1648.422305	19.612851
56.889918	1643.313496	19.617869
57.151625	1649.508741	19.622887
56.860541	1657.137074	19.627904
57.084155	1652.494057	19.632922
57.262394	1662.737393	19.637939
56.962440	1651.973917	19.642957
57.130222	1654.800597	19.647975
56.843284	1653.698056	19.652992
57.350262	1649.412538	19.658010
57.310030	1651.567683	19.663027
57.309945	1654.103387	19.668045
57.630851	1663.646003	19.673063
57.624939	1681.132558	19.678080
57.871429	1673.660752	19.683098
57.742858	1679.896231	19.688115
58.012559	1682.552506	19.693133
57.924141	1683.038507	19.698151
57.931130	1682.202118	19.703168
58.023050	1672.654990	19.708186
58.069853	1671.481918	19.713203
58.111661	1670.529865	19.718221
58.528087	1673.684980	19.723239
57.832941	1663.052161	19.728256
57.997045	1659.211430	19.733274
58.582732	1670.341464	19.738291
58.083552	1673.740128	19.743309
58.385018	1669.891645	19.748327
58.431950	1677.091704	19.753344
58.598212	1663.861311	19.758362
58.658247	1672.020388	19.763379
58.646295	1665.604397	19.768397
59.235269	1655.842729	19.773415
58.764580	1674.833268	19.778432
58.776191	1669.442269	19.783450
58.873224	1675.408959	19.788467
58.391216	1676.047392	19.793485
58.825670	1662.906362	19.798503
58.933880	1667.853528	19.803520
58.985968	1670.915738	19.808538
58.833687	1676.346467	19.813555
58.820610	1681.427811	19.818573
59.072630	1666.805778	19.823591
59.161259	1681.834368	19.828608
59.398892	1685.337321	19.833626
59.575776	1692.741604	19.838643
59.340056	1681.360677	19.843661
59.486406	1686.059523	19.848679
59.452405	1693.462832	19.853696
59.629210	1691.193083	19.858714
59.254004	1698.949684	19.863731
59.273592	1699.835310	19.868749
59.749588	1692.314308	19.873767
59.206089	1699.196411	19.878784
59.378737	1702.000302	19.883802
59.680799	1698.478904	19.888819
59.593098	1716.239666	19.893837
59.833232	1714.732166	19.898855
59.923933	1730.293728	19.903872
60.228329	1722.013569	19.908890
59.988621	1720.345069	19.913907
60.073695	1723.620679	19.918925
60.508620	1722.017619	19.923943
60.355512	1721.353050	19.928960
60.532041	1706.036732	19.933978
60.644084	1716.197856	19.938995
60.279388	1723.940209	19.944013
60.368064	1724.207633	19.949031
60.574311	1733.645887	19.954048
60.677877	1741.958509	19.959066
60.720519	1740.970139	19.964083
60.515947	1748.499779	19.969101
60.817098	1734.119954	19.974119
61.031615	1733.476980	19.979136
60.935859	1726.714105	19.984154
61.334548	1733.496299	19.989171
61.541969	1737.485428	19.994189
61.725615	1724.854674	19.999207
61.744239	1734.547792	20.004224
61.670616	1726.080953	20.009242
61.788459	1723.781278	20.014259
61.533004	1732.500362	20.019277
61.821420	1714.158578	20.024295
61.529402	1719.512508	20.029312
61.576288	1716.991343	20.034330
61.944005	1707.041560	20.039347
61.758124	1729.098176	20.044365
61.936250	1724.832050	20.049383
62.040956	1726.522073	20.054400
61.867045	1720.647837	20.059418
61.876523	1725.834137	20.064435
61.632491	1727.040232	20.069453
61.914490	1717.196920	20.074471
61.631673	1735.542525	20.079488
61.962489	1715.396016	20.084506
61.856255	1722.058956	20.089523
61.984656	1733.145564	20.094541
62.058685	1718.880627	20.099559
61.965755	1745.786218	20.104576
62.195716	1753.576896	20.109594
62.450601	1749.314251	20.114611
62.494813	1748.396417	20.119629
62.835542	1757.305153	20.124647
62.378009	1763.687511	20.129664
62.373588	1760.551604	20.134682
62.787783	1741.398496	20.139699
62.581331	1778.705767	20.144717
62.915492	1788.996686	20.149735
62.788178	1792.095398	20.154752
62.631221	1764.203953	20.159770
62.956289	1780.928410	20.164787
62.792660	1792.527252	20.169805
63.279969	1780.126448	20.174823
63.201200	1785.576955	20.179840
63.331188	1795.485161	20.184858
63.615478	1806.661795	20.189875
63.663756	1813.050025	20.194893
63.714332	1806.161529	20.199911
63.609408	1812.062956	20.204928
63.764873	1805.407845	20.209946
63.813545	1801.404588	20.214963
63.910028	1815.555888	20.219981
64.102121	1802.374733	20.224999
63.952582	1795.072990	20.230016
64.206761	1786.987993	20.235034
64.580971	1796.594557	20.240051
64.133324	1774.522461	20.245069
64.213788	1761.525886	20.250087
64.134624	1776.144033	20.255104
64.337261	1782.490329	20.260122
64.173234	1775.102817	20.265139
64.420029	1786.776199	20.270157
64.805191	1776.117298	20.275175
64.768149	1786.903144	20.280192
64.403822	1784.274514	20.285210
64.716062	1784.938868	20.290227
64.557891	1783.367467	20.295245
64.387906	1788.679939	20.300263
64.227616	1792.768624	20.305280
64.195809	1791.949426	20.310298
64.705769	1794.207184	20.315315
64.826354	1801.225672	20.320333
64.946451	1795.515303	20.325351
65.091334	1798.773527	20.330368
64.934624	1804.783884	20.335386
65.255240	1805.000163	20.340403
65.040563	1820.484682	20.345421
65.448934	1829.757057	20.350439
65.501423	1837.110466	20.355456
65.610530	1838.258677	20.360474
66.031301	1831.194727	20.365491
65.756929	1829.387022	20.370509
66.006247	1831.120062	20.375527
65.875043	1820.519884	20.380544
65.715477	1812.491418	20.385562
65.850552	1820.817937	20.390579
65.945350	1822.833596	20.395597
65.834853	1835.951411	20.400615
66.008427	1830.021714	20.405632
66.067001	1831.829218	20.410650
66.589589	1829.656888	20.415667
66.156961	1838.685863	20.420685
66.383496	1835.763218	20.425703
66.097969	1831.267409	20.430720
66.406807	1828.520405	20.435738
66.555140	1826.554052	20.440755
66.214179	1828.917632	20.445773
66.617554	1823.728366	20.450791
66.461097	1826.902519	20.455808
66.566848	1846.605170	20.460826
66.547231	1853.024694	20.465843
66.361527	1861.336326	20.470861
66.708250	1856.283499	20.475879
66.718073	1863.395187	20.480896
66.707275	1863.799601	20.485914
66.923491	1866.719274	20.490931
67.040687	1883.772732	20.495949
67.450411	1889.779307	20.500967
67.547180	1883.913747	20.505984
67.303639	1888.033039	20.511002
67.277518	1878.597410	20.516019
67.373475	1881.306600	20.521037
67.608447	1883.968453	20.526055
67.593882	1875.388288	20.531072
67.461524	1889.796381	20.536090
67.473872	1889.410586	20.541107
67.832559	1906.636346	20.546125
67.914946	1902.973753	20.551143
68.005245	1904.463173	20.556160
67.851308	1906.265252	20.561178
68.280713	1910.617007	20.566195
68.035860	1908.150200	20.571213
68.295875	1904.701527	20.576231
68.466361	1901.006008	20.581248
68.443210	1910.331523	20.586266
68.763090	1893.312141	20.591283
68.551244	1900.825716	20.596301
68.578866	1899.336359	20.601319
68.599959	1900.391645	20.606336
68.323636	1894.186029	20.611354
68.888983	1908.045567	20.616371
68.729610	1933.999403	20.621389
68.980247	1925.173993	20.626407
69.110743	1928.200157	20.631424
69.001688	1929.335977	20.636442
69.448867	1926.351386	20.641459
69.397981	1933.623801	20.646477
69.381656	1932.607070	20.651495
69.511488	1936.640089	20.656512
69.335683	1931.170341	20.661530
69.809514	1922.087538	20.666547
69.576763	1929.439293	20.671565
69.529335	1929.025277	20.676583
69.641697	1920.349337	20.681600
69.423045	1919.806897	20.686618
69.485092	1927.374334	20.691635
69.600126	1909.753666	20.696653
69.545603	1921.311615	20.701671
69.754041	1922.555678	20.706688
69.536501	1927.676008	20.711706
70.186396	1940.771754	20.716723
70.167580	1953.322915	20.721741
70.430411	1961.531613	20.726759
70.396351	1949.430893	20.731776
70.413339	1953.035168	20.736794
70.435605	1955.987363	20.741811
70.376898	1946.950147	20.746829
70.402033	1930.863350	20.751847
70.623451	1934.480637	20.756864
70.296108	1944.354913	20.761882
70.460971	1940.611517	20.766899
70.678536	1957.413099	20.771917
70.682789	1963.171333	20.776935
71.112779	1967.875374	20.781952
70.981994	1973.773126	20.786970
71.243847	1963.876232	20.791987
71.395048	1963.693237	20.797005
71.551738	1971.111895	20.802023
71.907752	1966.694633	20.807040
71.347533	1968.224880	20.812058
71.940553	1960.990251	20.817075
71.505218	1965.523974	20.822093
71.552620	1964.674831	20.827111
71.879110	1959.689691	20.832128
71.607039	1966.618293	20.837146
71.916381	1960.681048	20.842163
72.181600	1959.153794	20.847181
71.797045	1963.880768	20.852199
72.121685	1970.270612	20.857216
72.168331	1970.565193	20.862234
72.468643	1956.271801	20.867251
72.077111	1958.100765	20.872269
71.756745	1969.641373	20.877287
71.825393	1963.536443	20.882304
71.705718	1984.431419	20.887322
71.851673	1986.077142	20.892339
72.136566	2003.715913	20.897357
72.019566	2007.089882	20.902375
72.297089	2011.409260	20.907392
72.442514	2023.654287	20.912410
73.070736	2016.963012	20.917427
73.010435	2016.459810	20.922445
72.648377	2022.602106	20.927463
73.215127	2020.899341	20.932480
72.932219	2012.410654	20.937498
73.127634	2018.703149	20.942515
73.302482	2016.977939	20.947533
73.312108	2024.390189	20.952551
73.771534	2015.116142	20.957568
73.572256	2021.940352	20.962586
73.350621	2014.889099	20.967603
73.913897	2013.556555	20.972621
73.842464	2028.695977	20.977639
74.123288	2026.793413	20.982656
73.795952	2017.053367	20.987674
74.032005	2007.077186	20.992691
73.998877	2009.479793	20.997709
74.169551	2010.407412	21.002727
74.431790	2020.749294	21.007744
74.058336	2029.460630	21.012762
74.393073	2023.008069	21.017779
74.777684	2027.922291	21.022797
74.315974	2018.530868	21.027815
74.515028	2011.966240	21.032832
74.265398	2038.758936	21.037850
74.396672	2029.595415	21.042867
74.663553	2029.230373	21.047885
74.433484	2026.385228	21.052903
74.727864	2019.863598	21.057920
74.431146	2033.519384	21.062938
74.837107	2040.366634	21.067955
75.008089	2045.727071	21.072973
74.988965	2059.969407	21.077991
75.161288	2046.157243	21.083008
75.038071	2056.497699	21.088026
75.278400	2049.839954	21.093043
75.278874	2057.651664	21.098061
75.327756	2060.683007	21.103079
75.910951	2048.773210	21.108096
75.387964	2057.532006	21.113114
75.440557	2047.594493	21.118131
75.541568	2064.696365	21.123149
75.654209	2070.297354	21.128167
75.903978	2077.499872	21.133184
75.900179	2080.766141	21.138202
76.144332	2076.887367	21.143219
76.303797	2078.886457	21.148237
76.391362	2088.199149	21.153255
76.149583	2073.705795	21.158272
76.575506	2074.805075	21.163290
76.588135	2073.994505	21.168307
76.673444	2075.708113	21.173325
76.291822	2077.194158	21.178343
76.636065	2067.367427	21.183360
76.566904	2075.390030	21.188378
76.439594	2077.238220	21.193395
76.755411	2103.135454	21.198413
76.568263	2114.837406	21.203431
76.963457	2097.602851	21.208448
77.000286	2101.756143	21.213466
77.018189	2107.649114	21.218483
77.382247	2104.534595	21.223501
77.393034	2096.719482	21.228519
77.558861	2097.652599	21.233536
77.575758	2100.171515	21.238554
77.741059	2092.105243	21.243571
77.906738	2096.936424	21.248589
77.458897	2102.021180	21.253607
77.939464	2092.572249	21.258624
77.534523	2097.551060	21.263642
77.654475	2096.975063	21.268659
77.879792	2102.051570	21.273677
77.962810	2125.602785	21.278695
78.170961	2117.506069	21.283712
78.087034	2120.962881	21.288730
77.911305	2119.034012	21.293747
78.119888	2115.181351	21.298765
77.886497	2125.929545	21.303783
78.233873	2119.934261	21.308800
78.473730	2133.591089	21.313818
78.421458	2150.305363	21.318835
78.698627	2147.833918	21.323853
78.687739	2149.597483	21.328871
78.828824	2146.389523	21.333888
78.922099	2144.606519	21.338906
78.498815	2156.558526	21.343923
78.899972	2148.665400	21.348941
78.993810	2161.945983	21.353959
79.140155	2169.135152	21.358976
79.014639	2170.710928	21.363994
78.903911	2178.040201	21.369011
79.126917	2164.581648	21.374029
79.529185	2192.964859	21.379047
79.604247	2186.942186	21.384064
79.976942	2196.465887	21.389082
80.108259	2189.694899	21.394099
80.286035	2184.771153	21.399117
79.828545	2195.893346	21.404135
80.180858	2192.220670	21.409152
80.285905	2189.743632	21.414170
80.152631	2193.275973	21.419187
80.369802	2188.660557	21.424205
80.295162	2185.391034	21.429223
80.393753	2184.124717	21.434240
80.294843	2188.241477	21.439258
80.102283	2192.217439	21.444275
80.426199	2186.268342	21.449293
80.386962	2200.372447	21.454311
80.454521	2209.392670	21.459328
80.924786	2200.876572	21.464346
80.741852	2209.858088	21.469363
80.748413	2204.774444	21.474381
80.659459	2209.721777	21.479399
80.893731	2213.481808	21.484416
80.976187	2234.215130	21.489434
81.336418	2235.691426	21.494451
81.661143	2239.540862	21.499469
81.497328	2242.816168	21.504487
81.880252	2231.952008	21.509504
81.844427	2239.661849	21.514522
81.879957	2245.786453	21.519539
81.659043	2238.845090	21.524557
81.388646	2234.635399	21.529575
81.930704	2238.566584	21.534592
82.010138	2246.738622	21.539610
82.092575	2238.114458	21.544627
82.306673	2229.589643	21.549645
82.087730	2245.374177	21.554663
82.468273	2247.915354	21.559680
82.497255	2248.041293	21.564698
82.478446	2264.255630	21.569715
82.689173	2254.715916	21.574733
82.698866	2259.580679	21.579751
82.624623	2255.705441	21.584768
82.948195	2253.960420	21.589786
82.711073	2259.328600	21.594803
83.071383	2253.346143	21.599821
82.581610	2258.266960	21.604839
82.523995	2269.605448	21.609856
83.156998	2277.784396	21.614874
83.148615	2286.772732	21.619891
83.194332	2281.135385	21.624909
83.186462	2291.793465	21.629927
83.341535	2283.318145	21.634944
83.644720	2294.096516	21.639962
83.676807	2315.233615	21.644979
84.140607	2304.284929	21.649997
84.026938	2316.065776	21.655015
84.379329	2312.291594	21.660032
84.540001	2300.232676	21.665050
84.615933	2301.467230	21.670067
84.474086	2280.024377	21.675085
84.333603	2272.433074	21.680103
84.141807	2270.344719	21.685120
84.624448	2287.178348	21.690138
84.645560	2305.351928	21.695155
85.060979	2288.122575	21.700173
84.815739	2294.765472	21.705191
84.750571	2304.078276	21.710208
85.107851	2294.124255	21.715226
85.237153	2305.106549	21.720243
85.126938	2298.182898	21.725261
85.078941	2305.968650	21.730279
85.094644	2296.828111	21.735296
85.117823	2294.729066	21.740314
84.982071	2297.111118	21.745331
85.179811	2285.214621	21.750349
85.293214	2301.919953	21.755367
85.479807	2292.218890	21.760384
85.464802	2313.689125	21.765402
85.287341	2318.041826	21.770419
85.533310	2320.009851	21.775437
85.415136	2328.819086	21.780455
85.402507	2324.646916	21.785472
85.938350	2340.470069	21.790490
85.599229	2358.334632	21.795507
85.930418	2340.161427	21.800525
86.121966	2351.118885	21.805543
85.881480	2348.106229	21.810560
86.579800	2361.426669	21.815578
86.861130	2358.801150	21.820595
87.210054	2357.843337	21.825613
87.117990	2369.946412	21.830631
87.268368	2357.570537	21.835648
87.285113	2338.280248	21.840666
87.136304	2333.502918	21.845683
87.175726	2331.282510	21.850701
86.955766	2331.453654	21.855719
87.402513	2347.585190	21.860736
87.417179	2358.384450	21.865754
87.413169	2363.195588	21.870771
87.485840	2352.230585	21.875789
87.647968	2360.011173	21.880807
87.607936	2367.972660	21.885824
87.816470	2355.644931	21.890842
87.706495	2353.253281	21.895859
87.507677	2350.775909	21.900877
87.784460	2368.513164	21.905895
87.766943	2365.623830	21.910912
88.197542	2386.636133	21.915930
87.918055	2392.505854	21.920947
88.046119	2383.327679	21.925965
88.072772	2391.883398	21.930983
88.406147	2419.386884	21.936000
88.629037	2415.923564	21.941018
88.626980	2417.774632	21.946035
88.813012	2406.482399	21.951053
89.042457	2421.253336	21.956071
89.180010	2413.618407	21.961088
89.039647	2404.612018	21.966106
88.851309	2414.416463	21.971123
88.932422	2413.928449	21.976141
89.247148	2424.384952	21.981159
89.470670	2432.210847	21.986176
89.826595	2437.799138	21.991194
89.677580	2443.126593	21.996211
90.157939	2440.183017	22.001229
90.071506	2437.627930	22.006247
89.945416	2440.057230	22.011264
90.142928	2426.069223	22.016282
90.101687	2434.635008	22.021299
90.097489	2418.913374	22.026317
90.206951	2431.800798	22.031335
90.349208	2423.163052	22.036352
90.568404	2410.607051	22.041370
90.302657	2421.366128	22.046387
90.833241	2424.371856	22.051405
90.449013	2419.946659	22.056423
90.278948	2424.103934	22.061440
90.374251	2415.586943	22.066458
90.482730	2423.841757	22.071475
90.655719	2438.438450	22.076493
90.542777	2447.884026	22.081511
90.711293	2458.238808	22.086528
91.335125	2439.965326	22.091546
90.860386	2462.469470	22.096563
91.076644	2451.917243	22.101581
91.447048	2475.983219	22.106599
91.681467	2477.102062	22.111616
91.812006	2475.200599	22.116634
91.629811	2480.589989	22.121651
92.053213	2468.441842	22.126669
91.934297	2485.713782	22.131687
91.953934	2474.287574	22.136704
92.308716	2465.699286	22.141722
92.013393	2475.957368	22.146739
92.043403	2464.734016	22.151757
92.562037	2488.304446	22.156775
92.603542	2503.747263	22.161792
92.674431	2497.935923	22.166810
92.772467	2506.098063	22.171827
92.949142	2501.644744	22.176845
92.696175	2501.604065	22.181863
92.950350	2496.059241	22.186880
93.360524	2495.388183	22.191898
93.150838	2503.243085	22.196915
93.218903	2495.587732	22.201933
93.080256	2501.118844	22.206951
93.111885	2493.564476	22.211968
93.334155	2497.175478	22.216986
93.492718	2514.043749	22.222003
93.579177	2509.133670	22.227021
93.498616	2519.720921	22.232039
93.561254	2514.165734	22.237056
93.923976	2510.697397	22.242074
93.563648	2526.375786	22.247091
93.736493	2542.422224	22.252109
94.126904	2532.513884	22.257127
93.951419	2542.427269	22.262144
94.406223	2547.613638	22.267162
93.952203	2549.729503	22.272179
94.144206	2557.565997	22.277197
94.587451	2570.470321	22.282215
94.330528	2575.196012	22.287232
94.741007	2561.823608	22.292250
94.839814	2576.167200	22.297267
95.006941	2573.938975	22.302285
95.261293	2564.458174	22.307303
95.080549	2565.194106	22.312320
95.057982	2574.854239	22.317338
95.177069	2592.757711	22.322355
95.365275	2590.431735	22.327373
95.538860	2591.890642	22.332391
95.949106	2587.450390	22.337408
95.967043	2590.845449	22.342426
95.996640	2591.270185	22.347443
95.938146	2599.034170	22.352461
96.199785	2595.659802	22.357479
96.198623	2599.828734	22.362496
96.249850	2587.074412	22.367514
96.087965	2589.846877	22.372531
96.188373	2587.070835	22.377549
96.466594	2594.086595	22.382567
96.729411	2596.275355	22.387584
97.077742	2606.052552	22.392602
97.146076	2611.463391	22.397619
96.478657	2603.811216	22.402637
96.770832	2608.052143	22.407655
96.721629	2609.086442	22.412672
97.001342	2602.821739	22.417690
97.243610	2615.328692	22.422707
97.256866	2614.797220	22.427725
97.702335	2602.305651	22.432743
97.242878	2627.337178	22.437760
97.758145	2630.326517	22.442778
97.687220	2634.881772	22.447795
97.853908	2644.346595	22.452813
97.859427	2639.616130	22.457831
97.975850	2646.866941	22.462848
97.867375	2634.840441	22.467866
97.792016	2644.888948	22.472883
97.771909	2654.494470	22.477901
98.258903	2652.566818	22.482919
98.293185	2672.833366	22.487936
98.736308	2668.801579	22.492954
98.639323	2662.633102	22.497971
98.645037	2661.280875	22.502989
99.136477	2661.193851	22.508007
98.844835	2674.423109	22.513024
99.148113	2678.994216	22.518042
99.170712	2692.473059	22.523059
99.342903	2688.703922	22.528077
99.662583	2684.346515	22.533095
99.409856	2702.291322	22.538112
99.662564	2685.516913	22.543130
100.152977	2684.542025	22.548147
99.858508	2699.602085	22.553165
99.941908	2683.413137	22.558183
99.789828	2682.344063	22.563200
100.132405	2682.483711	22.568218
99.966342	2679.333267	22.573235
99.877585	2686.413097	22.578253
99.885650	2686.398435	22.583271
99.913253	2693.519492	22.588288
100.291208	2701.287084	22.593306
100.232917	2711.190547	22.598323
100.165717	2712.548641	22.603341
100.439216	2708.362197	22.608359
100.512903	2726.484658	22.613376
100.819426	2739.615442	22.618394
100.687519	2743.494572	22.623411
101.024427	2732.632661	22.628429
101.184031	2745.489558	22.633447
100.987318	2755.712446	22.638464
101.433112	2766.016940	22.643482
101.416634	2762.775766	22.648499
101.525678	2761.616280	22.653517
101.666233	2760.473793	22.658535
101.583777	2770.252152	22.663552
101.882600	2770.562384	22.668570
102.080834	2794.694887	22.673587
102.125902	2801.071478	22.678605
102.731921	2786.601103	22.683623
102.624628	2794.822105	22.688640
102.861660	2783.438858	22.693658
102.839539	2777.726401	22.698675
102.724466	2784.263025	22.703693
102.961861	2778.454125	22.708711
103.010489	2784.336178	22.713728
103.111148	2778.737858	22.718746
103.043852	2785.139440	22.723763
102.877178	2781.684669	22.728781
103.245288	2774.990489	22.733799
103.119657	2782.826630	22.738816
103.037478	2799.530688	22.743834
103.419882	2803.021057	22.748851
103.883250	2805.080335	22.753869
103.743033	2811.749192	22.758887
103.512299	2811.055259	22.763904
103.819712	2798.357434	22.768922
103.839313	2827.400702	22.773939
103.632252	2838.600644	22.778957
104.166651	2834.684828	22.783975
104.136937	2836.801502	22.788992
104.294913	2839.884830	22.794010
104.639146	2847.330665	22.799027
104.423806	2860.050811	22.804045
104.675175	2863.688728	22.809063
104.464808	2860.301472	22.814080
104.880631	2854.802315	22.819098
105.176781	2868.969998	22.824115
105.407963	2890.952426	22.829133
105.780159	2868.280698	22.834151
105.704004	2884.428573	22.839168
105.831912	2885.309584	22.844186
105.958572	2862.363963	22.849203
105.849664	2859.555962	22.854221
105.500314	2849.978535	22.859239
105.897991	2858.506827	22.864256
106.132580	2871.653922	22.869274
106.027605	2876.357051	22.874291
105.831705	2879.213652	22.879309
106.454457	2866.360083	22.884327
106.351688	2877.517467	22.889344
106.264466	2872.468995	22.894362
106.332847	2876.591521	22.899379
106.492168	2893.560793	22.904397
106.326796	2890.576159	22.909415
106.024767	2903.598838	22.914432
106.430050	2922.649523	22.919450
106.421227	2926.178712	22.924467
106.503909	2924.554618	22.929485
107.057348	2949.367756	22.934503
107.430189	2953.894035	22.939520
107.380275	2962.122499	22.944538
107.959635	2952.566810	22.949555
107.989098	2956.873331	22.954573
107.946644	2939.101913	22.959591
107.787931	2952.968588	22.964608
108.357790	2955.360147	22.969626
108.253283	2949.555359	22.974643
108.074234	2956.266655	22.979661
108.503753	2974.121881	22.984679
108.499794	2976.405155	22.989696
108.558987	2979.755183	22.994714
108.939158	2980.529902	22.999731
108.817839	2978.151755	23.004749
108.868097	2980.343007	23.009767
108.694020	2972.172267	23.014784
108.886000	2994.774633	23.019802
109.287671	2998.491660	23.024819
109.242466	3011.831375	23.029837
109.531815	3005.703402	23.034855
109.865918	3004.025049	23.039872
109.644128	2986.090245	23.044890
109.589268	2994.462673	23.049907
109.627317	3016.378552	23.054925
109.992749	3023.567820	23.059943
110.121989	3026.113031	23.064960
110.451523	3024.009865	23.069978
110.789186	3014.491892	23.074995
110.844714	3034.418899	23.080013
110.707719	3022.721483	23.085031
110.904273	3012.680126	23.090048
110.498812	3025.639175	23.095066
110.858209	3017.482450	23.100083
110.465469	3018.514925	23.105101
110.954244	3022.534274	23.110119
111.002088	3041.856063	23.115136
111.281204	3043.889698	23.120154
111.893621	3032.038164	23.125171
111.988353	3045.228169	23.130189
111.760883	3046.916257	23.135207
111.768443	3041.544273	23.140224
111.722909	3043.134130	23.145242
111.912440	3047.409647	23.150259
111.853729	3053.043060	23.155277
111.954276	3053.749891	23.160295
112.231528	3052.487262	23.165312
112.129788	3053.507159	23.170330
112.309440	3077.650960	23.175347
112.505721	3079.048878	23.180365
112.705353	3071.697103	23.185383
112.403685	3073.128014	23.190400
112.540649	3072.545336	23.195418
112.635610	3076.816278	23.200435
112.958619	3088.285847	23.205453
113.118313	3093.681511	23.210471
113.339555	3096.452758	23.215488
113.240537	3101.920356	23.220506
113.393668	3103.787668	23.225523
113.289551	3120.654481	23.230541
113.335479	3130.634426	23.235559
113.533596	3134.151904	23.240576
113.653879	3136.800819	23.245594
113.837061	3145.802400	23.250611
113.723312	3156.441813	23.255629
114.262198	3145.790447	23.260647
114.382501	3150.858901	23.265664
114.451688	3172.138420	23.270682
114.973880	3170.864254	23.275699
114.928570	3180.687306	23.280717
115.005565	3174.215563	23.285735
115.436925	3174.619514	23.290752
115.240546	3179.404962	23.295770
115.359853	3176.186093	23.300787
115.168020	3183.881193	23.305805
115.729929	3165.302052	23.310823
115.880547	3169.756860	23.315840
115.622339	3169.016161	23.320858
115.868799	3182.576176	23.325875
115.808685	3181.759053	23.330893
115.853785	3195.444007	23.335911
115.850408	3194.396804	23.340928
116.082259	3193.349062	23.345946
116.403298	3182.096057	23.350963
116.195596	3204.035674	23.355981
116.770686	3210.806175	23.360999
116.604737	3217.249635	23.366016
116.482823	3226.784455	23.371034
117.043787	3215.768473	23.376051
117.231118	3216.040648	23.381069
117.172760	3208.888834	23.386087
117.577207	3235.383566	23.391104
117.415387	3239.242424	23.396122
117.904707	3235.127608	23.401139
117.669539	3249.687156	23.406157
117.928820	3237.703773	23.411175
117.992979	3242.109463	23.416192
117.822766	3240.311708	23.421210
118.308874	3228.817606	23.426227
118.243583	3233.393387	23.431245
117.943682	3237.026486	23.436263
118.180907	3226.618239	23.441280
118.318710	3243.146139	23.446298
118.912857	3248.003776	23.451315
118.900508	3265.448426	23.456333
118.707111	3264.482647	23.461351
118.885810	3264.365263	23.466368
118.865889	3267.561215	23.471386
119.208891	3256.111936	23.476403
119.096083	3264.093383	23.481421
119.146196	3279.983222	23.486439
119.146274	3288.398186	23.491456
119.233006	3290.448375	23.496474
119.690576	3292.805984	23.501491
119.594852	3311.646030	23.506509
119.929487	3320.223979	23.511527
120.003736	3315.468177	23.516544
119.799334	3325.050825	23.521562
120.282366	3326.800274	23.526579
120.319276	3345.549207	23.531597
120.283557	3348.186066	23.536615
120.926896	3343.438621	23.541632
120.805367	3347.486160	23.546650
120.667087	3351.191053	23.551667
120.996842	3370.842746	23.556685
121.210526	3370.388625	23.561703
121.629056	3365.768266	23.566720
121.224042	3376.774429	23.571738
121.552366	3371.649297	23.576755
121.624875	3376.879624	23.581773
121.774566	3391.324456	23.586791
122.018921	3386.045162	23.591808
121.749438	3395.019967	23.596826
122.187950	3380.949356	23.601843
122.205637	3396.978215	23.606861
122.414808	3407.040871	23.611879
122.835028	3407.214560	23.616896
122.831161	3430.179203	23.621914
122.870655	3418.067893	23.626931
123.026095	3415.230218	23.631949
123.213367	3416.830189	23.636967
123.271990	3416.154586	23.641984
123.132396	3408.374548	23.647002
123.150714	3411.200239	23.652019
123.245228	3425.959105	23.657037
123.364757	3437.113719	23.662055
123.683284	3433.367468	23.667072
123.819831	3433.436150	23.672090
124.025432	3424.414865	23.677107
124.107058	3432.980522	23.682125
124.271701	3444.372581	23.687143
124.191188	3449.960854	23.692160
124.269058	3464.218200	23.697178
124.227780	3464.253096	23.702195
124.747713	3464.012078	23.707213
124.516225	3455.828982	23.712231
125.055948	3478.274391	23.717248
125.000336	3490.227845	23.722266
124.998066	3485.052344	23.727283
125.402840	3482.919813	23.732301
125.284904	3491.315168	23.737319
125.481956	3489.125299	23.742336
125.466267	3498.157236	23.747354
125.577859	3502.967622	23.752371
125.663647	3515.028340	23.757389
126.124759	3520.628601	23.762407
126.394269	3513.993861	23.767424
126.097614	3518.804847	23.772442
126.361243	3521.080936	23.777459
126.545432	3526.136188	23.782477
126.309557	3546.642892	23.787495
126.928021	3542.884972	23.792512
126.773416	3550.492520	23.797530
127.188991	3543.028203	23.802547
127.183087	3540.908446	23.807565
127.288217	3553.062077	23.812583
127.564402	3565.715470	23.817600
127.511993	3576.488570	23.822618
127.675471	3572.504280	23.827635
127.859135	3575.907754	23.832653
127.675366	3578.706704	23.837671
127.968617	3571.627651	23.842688
127.993575	3580.316489	23.847706
128.537461	3596.476407	23.852723
128.517284	3595.159688	23.857741
128.112044	3589.327869	23.862759
128.555140	3595.289727	23.867776
128.586004	3606.055077	23.872794
128.726176	3611.662499	23.877811
128.751198	3630.054998	23.882829
128.747443	3627.129394	23.887847
128.908122	3643.311137	23.892864
128.993539	3657.163149	23.897882
128.883815	3654.336245	23.902899
129.420778	3673.641448	23.907917
129.784662	3679.589227	23.912935
130.527073	3673.019814	23.917952
129.991762	3671.944910	23.922970
130.540584	3676.964885	23.927987
130.852564	3666.016588	23.933005
130.671635	3675.530433	23.938023
130.857820	3684.918884	23.943040
130.596875	3679.704325	23.948058
130.701618	3674.075908	23.953075
130.972012	3684.490836	23.958093
130.759113	3704.470998	23.963111
131.213305	3697.311160	23.968128
131.093641	3708.315333	23.973146
130.829327	3700.855513	23.978163
131.048061	3706.250644	23.983181
131.305340	3723.062885	23.988199
131.629892	3726.142654	23.993216
131.485769	3730.109732	23.998234
131.853071	3746.810849	24.003251
132.151962	3753.249645	24.008269
131.826648	3761.041060	24.013287
132.175152	3747.430465	24.018304
132.303768	3768.102760	24.023322
132.295442	3784.352512	24.028339
132.879442	3785.082980	24.033357
132.868800	3779.118942	24.038375
133.434584	3787.855393	24.043392
133.429970	3800.928983	24.048410
133.592632	3796.968361	24.053427
134.114776	3798.334844	24.058445
133.939394	3801.887656	24.063463
134.086660	3788.180106	24.068480
134.334752	3788.299440	24.073498
134.220551	3794.698716	24.078515
134.208593	3782.151654	24.083533
134.486496	3791.000874	24.088551
134.549386	3785.091971	24.093568
134.750778	3782.474233	24.098586
134.746579	3790.020165	24.103603
134.737564	3785.264115	24.108621
134.785241	3813.430145	24.113639
134.940380	3822.095223	24.118656
134.796440	3819.654467	24.123674
134.717480	3827.779495	24.128691
135.415020	3835.340991	24.133709
135.385249	3852.234549	24.138727
135.761188	3850.967132	24.143744
135.606720	3858.352203	24.148762
136.449126	3875.494526	24.153779
136.483790	3876.830978	24.158797
136.214084	3877.522157	24.163815
136.655684	3874.770920	24.168832
136.883850	3870.788821	24.173850
136.703551	3873.210480	24.178867
136.965842	3857.948245	24.183885
136.753415	3871.074699	24.188903
136.970545	3881.364535	24.193920
136.950353	3900.893392	24.198938
137.134168	3897.962999	24.203955
137.303803	3893.242931	24.208973
137.348677	3924.434202	24.213991
137.554391	3921.397263	24.219008
137.617169	3919.336510	24.224026
137.628169	3918.553630	24.229043
137.848161	3936.758888	24.234061
138.179732	3942.703275	24.239079
138.869781	3940.819394	24.244096
138.670398	3953.777077	24.249114
138.674180	3943.106626	24.254131
139.108424	3940.487131	24.259149
138.647316	3945.752402	24.264167
139.083732	3959.441753	24.269184
138.888529	3973.416686	24.274202
139.157146	3975.526073	24.279219
139.505473	3974.462068	24.284237
139.412476	3991.602644	24.289255
139.746219	3986.911444	24.294272
139.947292	3994.588371	24.299290
139.973141	4006.832110	24.304307
140.059101	3999.048831	24.309325
140.105100	4013.836479	24.314343
140.411395	4017.662591	24.319360
140.809684	4011.954988	24.324378
140.959256	4020.490491	24.329395
140.989326	4017.763154	24.334413
141.415932	4019.378523	24.339431
141.726182	4012.316216	24.344448
141.765402	4015.327482	24.349466
141.749875	4000.837032	24.354483
141.994473	4005.046629	24.359501
141.748159	4014.379179	24.364519
141.907359	4014.454480	24.369536
142.295242	4030.645264	24.374554
142.064242	4030.249443	24.379571
142.483952	4031.293244	24.384589
142.729607	4036.354607	24.389607
142.794632	4029.668071	24.394624
142.817409	4023.291915	24.399642
142.724178	4039.557061	24.404659
143.364455	4042.068953	24.409677
143.018698	4059.967322	24.414695
143.106491	4062.884323	24.419712
143.421642	4068.002267	24.424730
143.395638	4063.259848	24.429747
143.594269	4068.520658	24.434765
143.793468	4085.171878	24.439783
144.027487	4079.691034	24.444800
144.051641	4092.054684	24.449818
143.829880	4091.131128	24.454835
144.410132	4101.296357	24.459853
144.214577	4117.016245	24.464871
144.204768	4120.813337	24.469888
144.335239	4120.319759	24.474906
144.730091	4141.888592	24.479923
144.874863	4138.103006	24.484941
145.158586	4149.194226	24.489959
145.405797	4150.680887	24.494976
145.944437	4170.003004	24.499994
145.630625	4181.139964	24.505011
145.845447	4175.349062	24.510029
145.910918	4170.439415	24.515047
145.755970	4163.833517	24.520064
146.073251	4171.859370	24.525082
145.754465	4201.558744	24.530099
146.351825	4182.140404	24.535117
146.405790	4198.338204	24.540135
147.044309	4201.092692	24.545152
147.365825	4207.607535	24.550170
147.001552	4225.366674	24.555187
147.501624	4222.281167	24.560205
147.595431	4224.667045	24.565223
147.562525	4220.580163	24.570240
147.834514	4217.608903	24.575258
147.651621	4226.387903	24.580275
147.994604	4223.655475	24.585293
148.175187	4232.996401	24.590311
148.070982	4235.256523	24.595328
148.499256	4229.480338	24.600346
148.380386	4256.411211	24.605363
148.912248	4237.018975	24.610381
148.912181	4232.179542	24.615399
148.929910	4277.556745	24.620416
149.580761	4273.895748	24.625434
149.286687	4258.788672	24.630451
150.022653	4249.901793	24.635469
150.367231	4252.113961	24.640487
150.048308	4248.926973	24.645504
150.480448	4245.879039	24.650522
150.142922	4261.077359	24.655539
150.606741	4249.233604	24.660557
150.945908	4248.620216	24.665575
150.459433	4243.253404	24.670592
150.861508	4247.781727	24.675610
150.846594	4254.410805	24.680627
150.932634	4247.741272	24.685645
151.153266	4266.238686	24.690663
151.057117	4269.767176	24.695680
151.103924	4269.862759	24.700698
151.307803	4285.566339	24.705715
151.380344	4295.674207	24.710733
151.595393	4300.580066	24.715751
151.608258	4307.999254	24.720768
152.051441	4329.880826	24.725786
152.073725	4342.629657	24.730803
152.277375	4331.731181	24.735821
152.414932	4333.989743	24.740839
152.382022	4354.409360	24.745856
152.460252	4346.099287	24.750874
152.514728	4366.428682	24.755891
152.937592	4374.996337	24.760909
153.073075	4380.398700	24.765927
153.034171	4395.200271	24.770944
153.481970	4401.518856	24.775962
153.472092	4415.220010	24.780979
153.924620	4411.926503	24.785997
154.000722	4414.191729	24.791015
154.303837	4419.210238	24.796032
154.459234	4407.918205	24.801050
154.400070	4412.985034	24.806067
154.588610	4431.110965	24.811085
154.934933	4428.247383	24.816103
155.147770	4442.639922	24.821120
155.310408	4438.755439	24.826138
155.464954	4442.231412	24.831155
155.406522	4435.162395	24.836173
155.403371	4443.570671	24.841191
155.158084	4452.535179	24.846208
155.827036	4459.476174	24.851226
155.640391	4480.048703	24.856243
155.633270	4477.321704	24.861261
155.839713	4485.476322	24.866279
156.002830	4494.343485	24.871296
156.374611	4505.594002	24.876314
156.319369	4516.970039	24.881331
156.923143	4509.959028	24.886349
157.094161	4532.585998	24.891367
157.226642	4547.444569	24.896384
157.543465	4537.831394	24.901402
157.503176	4536.351811	24.906419
157.519946	4541.530870	24.911437
157.863540	4550.163186	24.916455
157.930429	4568.842827	24.921472
158.455401	4561.173333	24.926490
158.316683	4569.157259	24.931507
158.805707	4564.500121	24.936525
158.734574	4571.772355	24.941543
158.763714	4581.487716	24.946560
158.945177	4600.544821	24.951578
159.163451	4596.909452	24.956595
159.206086	4581.277145	24.961613
159.783229	4613.411612	24.966631
159.912537	4600.001955	24.971648
159.979638	4617.136615	24.976666
160.131155	4626.435228	24.981683
160.151233	4607.000600	24.986701
160.083899	4612.189948	24.991719
159.959439	4627.973778	24.996736
160.473339	4623.616309	25.001754
160.659975	4636.064645	25.006771
160.901031	4635.896407	25.011789
160.926060	4642.038638	25.016807
160.998157	4671.207783	25.021824
161.369022	4675.292031	25.026842
161.648134	4673.823655	25.031859
161.568014	4665.305008	25.036877
161.954468	4673.951019	25.041895
161.884176	4688.523462	25.046912
162.318643	4690.586060	25.051930
162.213538	4701.544602	25.056947
162.603716	4694.750068	25.061965
162.606508	4691.704421	25.066983
162.443768	4693.196716	25.072000
162.948027	4705.911498	25.077018
162.788052	4720.367684	25.082035
162.812911	4718.192505	25.087053
163.528328	4709.926955	25.092071
163.168923	4744.747258	25.097088
163.458298	4744.888344	25.102106
163.769340	4742.831161	25.107123
163.569047	4758.337726	25.112141
164.135580	4763.695893	25.117159
164.229414	4774.636144	25.122176
164.333440	4784.836090	25.127194
164.573630	4792.116224	25.132211
165.103667	4793.966145	25.137229
165.204421	4789.522671	25.142247
164.851408	4803.624246	25.147264
165.727846	4797.678055	25.152282
165.580267	4793.346547	25.157299
165.460779	4795.464443	25.162317
166.002328	4808.058514	25.167335
165.893132	4821.535159	25.172352
166.324029	4821.676496	25.177370
166.205835	4829.182137	25.182387
166.384729	4831.320905	25.187405
166.902116	4836.421039	25.192423
166.343172	4852.545786	25.197440
166.727348	4868.341607	25.202458
166.847556	4868.729150	25.207475
167.208384	4886.821882	25.212493
167.362096	4886.682515	25.217511
167.158221	4895.355910	25.222528
167.535480	4902.031315	25.227546
167.709009	4907.400274	25.232563
167.936210	4906.187958	25.237581
168.406476	4923.880961	25.242599
168.212508	4937.146236	25.247616
168.842590	4935.694253	25.252634
169.122745	4936.345009	25.257651
169.142788	4932.892994	25.262669
169.442585	4945.443127	25.267687
169.620483	4963.801125	25.272704
169.727546	4966.955961	25.277722
169.735861	4971.470985	25.282739
169.603781	4958.352056	25.287757
169.934543	4954.619998	25.292775
170.189967	4982.944743	25.297792
170.230312	4987.940837	25.302810
170.384504	4991.980265	25.307827
170.346548	4994.311755	25.312845
170.537594	5002.551719	25.317863
170.571350	5019.980878	25.322880
170.854254	5021.374620	25.327898
171.356650	5029.612160	25.332915
171.538785	5040.328485	25.337933
171.736973	5029.173118	25.342951
171.933421	5046.385205	25.347968
172.201901	5036.554422	25.352986
172.175355	5036.300617	25.358003
172.234707	5028.426633	25.363021
172.333800	5057.139896	25.368039
172.276718	5065.166928	25.373056
172.738535	5062.603423	25.378074
172.815724	5071.816619	25.383091
172.893329	5086.524788	25.388109
173.442831	5080.992490	25.393127
173.693992	5101.083072	25.398144
173.540257	5095.035896	25.403162
173.806376	5091.239374	25.408179
173.919928	5105.397440	25.413197
174.423438	5115.641703	25.418215
174.448227	5119.702585	25.423232
174.498619	5119.280746	25.428250
174.698346	5125.404767	25.433267
174.521224	5142.538855	25.438285
174.841814	5154.237797	25.443303
175.022038	5158.055207	25.448320
175.101259	5169.092485	25.453338
175.576422	5180.632279	25.458355
175.549421	5172.489563	25.463373
175.816117	5186.203195	25.468391
175.721835	5201.579254	25.473408
176.280894	5207.314820	25.478426
176.092185	5206.466948	25.483443
176.430291	5221.042462	25.488461
176.740334	5224.221634	25.493479
176.934736	5239.646110	25.498496
176.907727	5244.992884	25.503514
177.192206	5264.851021	25.508531
177.257110	5263.273563	25.513549
177.745834	5260.405216	25.518567
177.792847	5272.457042	25.523584
178.223009	5284.801021	25.528602
178.586618	5291.377297	25.533619
178.433377	5288.250199	25.538637
178.868003	5282.803799	25.543655
178.590120	5293.300998	25.548672
178.882886	5299.385084	25.553690
179.263021	5307.883006	25.558707
179.196465	5313.104730	25.563725
179.360788	5310.390365	25.568743
179.362636	5328.379603	25.573760
179.714062	5336.265343	25.578778
179.826822	5335.703749	25.583795
180.077464	5336.994101	25.588813
180.305361	5354.367530	25.593831
180.234632	5363.462099	25.598848
180.431289	5363.223837	25.603866
180.676657	5362.704037	25.608883
180.747025	5394.513502	25.613901
180.824330	5392.530473	25.618919
180.703742	5398.742651	25.623936
181.074357	5413.096042	25.628954
181.561916	5421.817637	25.633971
181.398833	5426.244480	25.638989
181.940599	5438.614852	25.644007
181.937375	5450.810148	25.649024
182.020737	5456.805745	25.654042
182.276591	5466.137819	25.659059
182.601426	5478.788263	25.664077
182.810137	5474.996864	25.669095
182.924359	5490.604316	25.674112
183.136336	5514.950744	25.679130
183.415715	5508.248244	25.684148
183.474577	5508.478017	25.689165
183.895737	5517.332982	25.694183
184.120648	5522.085846	25.699200
184.320213	5530.930519	25.704218
184.383934	5523.798233	25.709236
184.600478	5538.778934	25.714253
185.363806	5559.814365	25.719271
185.316963	5562.123759	25.724288
185.460723	5551.362167	25.729306
185.291530	5554.009686	25.734324
185.330407	5562.463038	25.739341
185.696501	5553.052191	25.744359
185.642098	5582.745236	25.749376
185.703544	5591.315374	25.754394
186.125239	5590.794990	25.759412
186.151499	5612.238305	25.764429
186.611153	5619.153441	25.769447
186.695787	5622.002028	25.774464
186.927728	5639.394031	25.779482
187.158231	5640.582987	25.784500
187.289502	5647.522956	25.789517
187.724747	5646.086241	25.794535
187.680999	5652.283128	25.799552
187.794885	5659.829289	25.804570
188.387559	5655.155293	25.809588
188.314897	5668.397164	25.814605
188.735290	5688.243647	25.819623
188.590508	5682.083873	25.824640
188.740463	5695.029084	25.829658
188.845215	5695.583540	25.834676
189.212487	5707.685365	25.839693
189.689213	5723.063765	25.844711
189.275520	5732.195144	25.849728
189.699258	5732.273129	25.854746
190.163101	5742.664194	25.859764
190.175064	5762.488566	25.864781
190.434813	5747.560718	25.869799
190.753764	5763.031185	25.874816
190.603658	5755.131204	25.879834
190.711160	5762.549412	25.884852
190.824332	5768.731558	25.889869
191.165052	5778.180111	25.894887
191.486058	5773.382604	25.899904
191.376954	5798.945047	25.904922
191.663435	5813.372035	25.909940
191.451585	5814.462383	25.914957
192.064589	5817.000980	25.919975
191.830986	5836.344572	25.924992
191.907950	5838.563466	25.930010
192.200310	5856.339458	25.935028
192.207631	5873.392277	25.940045
192.736904	5874.124521	25.945063
193.199581	5888.750858	25.950080
193.258691	5904.542190	25.955098
193.865418	5915.379493	25.960116
193.628574	5912.667610	25.965133
194.284325	5917.857000	25.970151
194.424134	5930.253322	25.975168
194.548271	5943.111606	25.980186
194.990427	5945.948101	25.985204
194.701590	5955.831500	25.990221
195.068725	5947.334427	25.995239
195.227241	5963.251587	26.000256
195.076819	5975.429873	26.005274
195.511134	5981.571138	26.010292
195.490085	5996.266047	26.015309
196.230003	5995.270867	26.020327
196.205068	5996.244101	26.025344
196.494947	6011.666753	26.030362
196.716866	6023.437980	26.035380
196.581695	6024.761580	26.040397
197.010699	6031.603913	26.045415
197.262967	6036.609848	26.050432
197.745796	6055.044114	26.055450
197.614432	6065.306078	26.060468
197.338992	6059.784569	26.065485
197.940888	6071.842996	26.070503
198.269299	6088.941644	26.075520
198.199246	6098.223015	26.080538
198.623880	6092.086368	26.085556
198.564992	6115.088367	26.090573
198.750092	6121.374847	26.095591
199.167228	6124.148493	26.100608
199.281431	6149.614575	26.105626
199.567950	6145.626503	26.110644
199.560806	6152.734325	26.115661
199.999950	6150.355208	26.120679
200.522344	6157.881343	26.125696
200.241934	6177.040089	26.130714
200.906561	6176.185143	26.135732
200.930780	6174.991713	26.140749
201.095768	6192.144071	26.145767
201.016083	6200.085633	26.150784
201.352414	6200.293998	26.155802
201.618075	6198.501909	26.160820
201.623828	6205.676935	26.165837
201.841758	6206.347902	26.170855
202.083923	6216.871417	26.175872
201.805690	6235.177053	26.180890
202.331595	6247.199748	26.185908
202.740617	6264.738132	26.190925
202.848667	6249.281663	26.195943
202.897610	6258.426150	26.200960
203.459749	6259.677156	26.205978
204.011785	6256.629380	26.210996
203.957649	6268.754006	26.216013
204.124287	6266.255457	26.221031
204.344889	6264.109424	26.226048
204.451236	6270.844384	26.231066
204.767838	6272.770232	26.236084
204.976491	6289.955867	26.241101
205.008821	6297.309227	26.246119
205.307661	6302.860918	26.251136
205.270994	6299.546652	26.256154
205.493680	6310.179551	26.261172
205.138866	6319.492296	26.266189
205.642518	6328.484875	26.271207
206.005408	6348.525519	26.276224
205.805597	6360.755266	26.281242
206.352354	6371.850299	26.286260
206.322005	6384.700553	26.291277
206.361167	6393.959191	26.296295
206.903045	6405.095152	26.301312
207.178628	6418.929681	26.306330
207.294150	6428.926737	26.311348
207.526574	6437.067287	26.316365
207.746221	6446.181530	26.321383
208.450684	6449.988874	26.326400
208.239373	6472.282464	26.331418
208.388390	6468.301279	26.336436
208.753494	6494.805825	26.341453
208.977465	6496.146955	26.346471
209.455803	6496.941644	26.351488
209.308969	6525.721361	26.356506
210.132716	6522.853659	26.361524
210.167284	6524.365818	26.366541
209.934052	6528.391118	26.371559
210.524290	6533.691097	26.376576
210.421984	6545.255582	26.381594
210.857135	6560.015221	26.386612
211.225029	6560.241378	26.391629
211.173204	6561.505319	26.396647
211.279984	6565.143622	26.401664
211.228423	6584.391506	26.406682
211.651266	6576.131456	26.411700
211.772172	6600.038655	26.416717
211.905265	6606.708923	26.421735
212.310850	6606.213110	26.426752
212.372232	6634.512959	26.431770
212.754703	6638.398435	26.436788
213.026813	6640.354243	26.441805
213.258663	6642.025362	26.446823
213.425123	6645.942917	26.451840
213.440574	6658.037098	26.456858
213.916469	6658.881754	26.461876
213.625652	6664.347413	26.466893
213.948412	6681.491710	26.471911
214.223755	6684.681458	26.476928
214.281658	6691.288221	26.481946
215.002756	6707.941828	26.486964
215.274502	6717.810321	26.491981
215.174276	6712.735059	26.496999
215.545245	6714.450098	26.502016
215.423788	6741.542485	26.507034
215.891138	6745.538771	26.512052
216.033879	6746.176905	26.517069
216.218051	6755.133346	26.522087
216.664204	6772.864685	26.527104
216.717045	6773.658773	26.532122
216.634489	6794.516903	26.537140
216.889874	6799.762572	26.542157
217.188543	6809.294026	26.547175
217.182235	6824.938627	26.552192
217.400435	6826.466389	26.557210
217.914384	6844.445072	26.562228
218.437454	6865.767733	26.567245
218.476502	6870.302829	26.572263
218.865912	6872.282455	26.577280
218.913032	6885.424493	26.582298
218.956512	6896.727614	26.587316
219.508685	6908.282462	26.592333
219.557761	6914.783729	26.597351
219.660629	6920.682398	26.602368
219.524679	6932.956723	26.607386
220.102135	6936.852110	26.612404
220.335525	6946.017187	26.617421
220.411827	6970.103614	26.622439
220.837441	6972.398494	26.627456
221.218290	6978.780809	26.632474
221.255543	6989.712842	26.637492
221.560909	7005.049093	26.642509
221.666782	6997.816538	26.647527
221.855694	7013.086388	26.652544
222.072094	7024.709017	26.657562
222.608077	7033.847155	26.662580
222.832822	7051.212860	26.667597
223.070729	7065.799884	26.672615
223.489729	7058.515022	26.677632
223.241747	7064.015698	26.682650
223.745228	7090.537021	26.687668
224.001393	7092.171271	26.692685
224.321298	7084.261741	26.697703
224.450808	7075.541481	26.702720
224.578806	7089.950925	26.707738
224.633862	7091.072771	26.712756
224.857283	7099.418904	26.717773
224.716998	7108.446951	26.722791
225.007395	7114.604559	26.727808
225.225656	7129.544116	26.732826
225.353187	7131.178421	26.737844
225.476034	7147.263837	26.742861
225.469144	7168.695810	26.747879
226.224462	7181.404199	26.752896
226.359912	7200.462563	26.757914
226.498977	7210.364340	26.762932
227.127900	7217.232798	26.767949
227.025693	7233.531215	26.772967
227.189910	7228.618189	26.777984
227.325941	7252.925301	26.783002
227.711987	7258.817517	26.788020
228.023620	7269.585636	26.793037
228.012929	7291.872077	26.798055
228.373043	7292.928787	26.803072
228.594547	7312.769826	26.808090
228.677705	7326.478520	26.813108
229.286926	7337.472272	26.818125
229.329998	7344.494766	26.823143
229.786203	7355.648256	26.828160
230.106979	7373.410533	26.833178
230.258252	7380.758846	26.838196
230.707744	7377.570623	26.843213
230.702601	7396.355023	26.848231
231.156995	7394.324205	26.853248
231.019887	7400.980468	26.858266
231.482122	7409.135278	26.863284
231.660015	7423.962759	26.868301
231.991484	7424.304109	26.873319
232.157321	7431.654847	26.878336
232.319405	7450.822588	26.883354
232.231201	7464.287274	26.888372
232.837921	7472.966712	26.893389
232.829786	7484.025941	26.898407
233.096737	7486.507494	26.903424
233.367447	7512.715760	26.908442
233.383284	7520.552316	26.913460
233.913187	7521.813302	26.918477
234.018210	7548.983573	26.923495
234.486191	7557.031328	26.928512
234.385277	7555.426557	26.933530
234.946256	7569.677749	26.938548
234.992357	7581.923588	26.943565
235.114926	7593.542738	26.948583
235.733573	7606.237090	26.953600
235.888446	7600.786457	26.958618
236.131772	7625.588512	26.963636
236.595136	7616.124671	26.968653
236.391364	7641.640860	26.973671
236.689911	7647.750969	26.978688
236.859636	7662.705883	26.983706
236.962840	7666.890300	26.988724
237.157476	7664.943344	26.993741
237.527535	7693.878187	26.998759
237.665283	7692.310105	27.003776
237.707735	7696.600995	27.008794
237.987522	7721.330516	27.013812
238.648130	7709.700504	27.018829
238.536506	7735.351661	27.023847
238.672021	7742.073201	27.028864
239.264082	7753.393389	27.033882
239.353407	7781.062290	27.038900
239.785631	7779.568431	27.043917
239.791558	7791.388088	27.048935
239.795588	7802.404699	27.053952
240.262909	7812.710130	27.058970
240.270216	7831.020205	27.063988
240.932896	7838.336008	27.069005
241.028952	7854.581468	27.074023
241.411977	7871.245437	27.079040
241.242738	7873.852454	27.084058
241.485468	7897.122296	27.089076
242.225999	7901.731581	27.094093
242.175133	7912.557166	27.099111
242.605809	7922.004564	27.104128
242.979484	7928.321556	27.109146
243.074587	7931.303471	27.114164
243.325851	7957.586831	27.119181
243.801349	7971.460190	27.124199
243.610865	7971.924888	27.129216
243.975496	7990.724270	27.134234
244.295646	7991.100489	27.139252
244.609307	8019.700320	27.144269
244.732459	8025.546625	27.149287
244.792592	8026.345126	27.154304
245.322168	8044.111907	27.159322
245.406597	8053.459573	27.164340
245.888213	8058.077133	27.169357
246.046755	8076.508183	27.174375
246.218524	8082.256273	27.179392
246.582013	8085.633713	27.184410
246.804541	8101.521725	27.189428
247.042016	8110.701825	27.194445
247.100783	8123.379646	27.199463
247.401309	8133.885783	27.204480
247.682109	8137.499096	27.209498
247.321186	8169.380909	27.214516
247.958527	8175.910919	27.219533
248.424476	8196.922784	27.224551
248.765661	8207.130569	27.229568
248.831787	8212.337669	27.234586
248.812024	8242.241391	27.239604
249.414826	8239.812265	27.244621
249.418010	8268.050537	27.249639
249.817380	8275.927073	27.254656
250.073501	8292.418963	27.259674
250.149678	8302.015963	27.264692
250.683329	8295.251230	27.269709
250.548156	8312.432644	27.274727
251.006246	8319.619994	27.279744
251.387748	8330.054349	27.284762
251.636135	8346.010892	27.289780
251.705166	8344.367142	27.294797
252.045436	8362.103891	27.299815
252.030965	8380.311099	27.304832
252.378780	8384.166374	27.309850
252.469153	8401.681765	27.314868
253.050273	8405.156782	27.319885
252.862810	8427.996368	27.324903
253.034650	8439.781437	27.329920
253.671265	8451.132044	27.334938
254.221656	8479.105658	27.339956
254.712359	8472.456281	27.344973
254.972041	8497.057318	27.349991
255.028152	8510.087623	27.355008
254.958062	8504.668587	27.360026
254.809583	8524.836971	27.365044
255.762431	8521.755555	27.370061
255.903610	8533.409457	27.375079
255.696851	8558.505923	27.380096
255.698486	8578.057935	27.385114
255.934627	8586.832514	27.390132
256.654452	8605.777498	27.395149
256.934108	8623.416418	27.400167
257.340306	8643.052748	27.405184
257.829111	8652.784854	27.410202
257.624268	8667.616356	27.415220
258.102559	8681.019381	27.420237
258.343712	8694.468874	27.425255
258.924667	8712.949051	27.430272
259.134416	8716.353504	27.435290
259.277711	8728.486433	27.440308
259.591934	8742.807206	27.445325
259.549287	8754.658189	27.450343
260.069645	8771.772623	27.455360
260.391003	8777.736352	27.460378
260.351114	8780.505465	27.465396
260.504064	8803.761133	27.470413
260.933697	8809.977913	27.475431
261.308279	8827.265943	27.480448
261.681626	8840.294757	27.485466
261.738334	8856.104563	27.490484
262.337649	8859.051148	27.495501
262.590992	8873.662671	27.500519
262.529499	8883.413400	27.505536
263.254375	8880.047596	27.510554
263.298985	8894.568869	27.515572
263.570303	8906.472616	27.520589
263.966161	8922.189875	27.525607
263.914183	8911.392140	27.530624
264.029661	8935.025400	27.535642
264.099324	8949.600569	27.540660
264.961257	8956.850158	27.545677
264.816638	8974.832930	27.550695
265.176215	8989.122711	27.555712
265.457425	8989.722352	27.560730
265.307385	9006.109018	27.565748
265.728652	9010.312756	27.570765
266.046974	9013.541413	27.575783
266.140345	9040.019854	27.580800
266.530709	9039.549226	27.585818
266.739560	9061.500362	27.590836
267.416501	9065.811301	27.595853
267.105684	9086.683447	27.600871
267.638509	9095.992952	27.605888
268.384117	9121.343813	27.610906
268.180044	9127.626720	27.615924
268.957212	9141.951596	27.620941
269.077252	9148.872179	27.625959
268.858342	9165.371507	27.630976
269.402294	9174.999166	27.635994
269.310740	9198.410884	27.641012
269.528353	9199.735578	27.646029
270.023316	9225.961086	27.651047
270.008621	9238.374571	27.656064
270.582683	9237.950989	27.661082
270.787840	9270.414968	27.666100
270.949564	9290.207189	27.671117
271.355610	9299.107768	27.676135
271.207803	9328.042954	27.681152
272.000881	9341.589984	27.686170
272.206366	9352.714518	27.691188
273.029052	9359.423657	27.696205
273.523119	9383.348246	27.701223
273.252955	9390.429501	27.706240
273.825561	9373.839310	27.711258
274.065896	9408.194453	27.716276
274.286839	9404.488254	27.721293
274.472766	9412.141308	27.726311
274.480151	9427.889545	27.731328
275.067676	9432.849498	27.736346
275.047207	9449.106219	27.741364
275.693222	9458.647366	27.746381
275.728776	9464.825330	27.751399
275.839629	9480.769993	27.756416
276.732191	9487.103708	27.761434
276.419881	9494.264126	27.766452
276.743097	9517.097550	27.771469
276.608385	9516.373406	27.776487
276.960971	9549.890613	27.781504
277.448972	9551.145487	27.786522
277.551581	9589.393499	27.791540
278.299609	9586.642382	27.796557
278.507052	9611.985428	27.801575
278.478318	9629.727813	27.806592
278.868704	9640.318274	27.811610
279.010991	9655.241003	27.816628
279.131082	9664.550551	27.821645
279.419752	9677.194620	27.826663
279.884604	9681.652867	27.831680
280.314648	9700.837846	27.836698
280.157620	9709.392066	27.841716
280.679635	9726.578161	27.846733
280.925523	9736.599160	27.851751
280.914331	9767.006629	27.856768
281.303450	9763.584771	27.861786
281.536638	9795.303732	27.866804
281.909417	9805.605556	27.871821
282.270592	9828.587253	27.876839
282.426759	9838.427852	27.881856
282.886908	9859.840398	27.886874
282.979352	9882.838255	27.891892
283.596598	9890.655350	27.896909
284.311102	9898.279492	27.901927
284.265001	9914.128837	27.906944
284.573768	9917.188449	27.911962
284.864608	9931.468843	27.916980
285.053827	9950.101923	27.921997
285.246894	9971.489915	27.927015
285.318455	9973.398660	27.932032
285.799958	9988.227126	27.937050
285.722112	10010.476388	27.942068
286.073881	10017.066119	27.947085
286.636528	10038.950888	27.952103
286.653040	10061.721888	27.957120
287.268619	10078.222599	27.962138
287.204735	10097.712276	27.967156
287.556096	10106.152244	27.972173
287.929306	10136.677045	27.977191
288.279099	10143.816837	27.982208
288.609073	10174.855014	27.987226
288.884679	10185.250892	27.992244
289.249670	10204.932835	27.997261
290.203279	10214.577722	28.002279
290.073636	10220.868106	28.007296
290.174417	10226.338346	28.012314
290.456449	10251.532473	28.017332
290.813696	10264.557624	28.022349
291.207982	10286.467623	28.027367
291.297437	10299.289953	28.032384
291.962435	10293.684247	28.037402
292.109528	10322.198961	28.042420
292.382612	10333.974505	28.047437
292.781784	10334.996894	28.052455
292.745455	10351.979951	28.057472
293.056066	10362.089818	28.062490
293.263217	10387.914667	28.067508
293.296755	10400.834531	28.072525
293.700349	10414.785774	28.077543
294.004062	10431.670653	28.082560
294.343716	10446.838547	28.087578
294.569055	10469.638265	28.092596
294.982379	10478.665489	28.097613
295.353075	10484.827052	28.102631
295.358535	10504.721333	28.107648
295.895037	10512.319863	28.112666
295.968850	10539.034260	28.117684
296.453527	10551.568738	28.122701
297.052312	10562.924638	28.127719
296.988800	10581.845503	28.132736
297.371031	10580.349518	28.137754
297.423013	10594.761872	28.142772
297.655264	10624.268562	28.147789
298.303134	10631.174172	28.152807
298.393744	10653.291686	28.157824
298.844520	10664.465850	28.162842
299.073704	10677.773052	28.167860
299.317768	10690.613572	28.172877
299.822270	10716.057517	28.177895
299.880273	10729.935464	28.182912
300.394825	10738.929005	28.187930
300.625062	10759.230872	28.192948
300.897819	10785.022338	28.197965
301.394771	10790.025914	28.202983
301.247404	10818.249307	28.208000
301.711105	10835.612424	28.213018
302.070515	10852.768676	28.218036
301.853260	10871.585734	28.223053
302.741192	10881.533109	28.228071
302.633217	10912.622938	28.233088
303.103544	10924.860958	28.238106
303.544018	10945.536447	28.243124
303.997986	10972.752942	28.248141
304.490209	10970.222585	28.253159
304.492054	10996.822950	28.258176
304.804858	11002.427706	28.263194
305.114470	11027.587653	28.268212
305.666178	11042.874246	28.273229
305.965746	11047.685860	28.278247
306.170188	11070.289133	28.283264
306.726139	11082.832373	28.288282
306.839459	11101.217693	28.293300
306.984463	11114.526893	28.298317
307.559714	11110.099576	28.303335
307.731928	11145.966050	28.308352
308.021554	11148.676390	28.313370
308.480061	11170.266970	28.318388
308.685060	11179.766974	28.323405
308.953560	11192.410031	28.328423
309.094021	11217.514225	28.333440
309.426689	11234.743056	28.338458
309.663641	11242.443613	28.343476
310.041682	11268.205748	28.348493
310.319095	11271.029814	28.353511
310.692129	11300.700735	28.358528
310.724269	11318.201663	28.363546
311.487329	11328.540322	28.368564
311.440423	11340.691121	28.373581
311.986477	11353.545072	28.378599
312.118157	11367.425636	28.383616
312.598473	11382.982099	28.388634
313.255161	11390.136540	28.393652
312.997069	11411.920378	28.398669
313.794784	11421.292229	28.403687
313.666687	11437.471840	28.408704
313.842087	11457.485500	28.413722
314.311026	11475.570228	28.418740
314.400579	11480.910100	28.423757
314.880931	11486.610718	28.428775
315.007544	11521.667632	28.433792
315.022215	11538.650979	28.438810
315.506808	11546.517246	28.443828
315.879071	11589.649461	28.448845
316.500170	11583.282536	28.453863
316.738480	11617.160995	28.458880
317.483606	11624.059442	28.463898
317.558169	11649.661639	28.468916
317.984582	11656.145756	28.473933
318.515047	11664.448665	28.478951
318.580526	11690.321545	28.483968
319.419201	11692.887421	28.488986
319.830283	11711.568785	28.494004
319.706933	11711.960709	28.499021
320.516472	11710.841196	28.504039
320.676064	11732.741128	28.509056
321.040686	11732.270210	28.514074
320.677587	11749.978657	28.519092
321.017679	11765.821917	28.524109
321.371740	11780.126659	28.529127
321.530450	11803.365595	28.534144
321.871009	11822.183869	28.539162
322.426438	11835.623090	28.544180
322.348413	11865.476410	28.549197
322.980309	11871.012930	28.554215
323.392664	11889.009973	28.559232
324.048479	11901.251501	28.564250
324.249521	11916.786520	28.569268
324.500126	11933.285665	28.574285
324.927183	11949.869648	28.579303
324.732091	11969.400361	28.584320
324.879298	11981.857992	28.589338
325.382639	11999.405032	28.594356
325.684694	12014.013824	28.599373
326.189095	12033.639743	28.604391
326.166203	12052.335205	28.609408
326.432958	12078.721513	28.614426
326.607776	12103.326644	28.619444
326.883664	12123.235644	28.624461
327.319898	12150.462999	28.629479
327.655648	12182.726115	28.634496
328.045339	12194.603186	28.639514
328.538810	12223.443101	28.644532
328.989717	12249.303917	28.649549
329.173214	12246.043362	28.654567
329.458806	12269.660852	28.659584
329.876746	12284.135738	28.664602
330.095417	12311.006488	28.669620
330.240382	12323.190463	28.674637
330.963356	12339.236780	28.679655
331.403829	12364.971754	28.684672
331.935471	12382.617640	28.689690
332.350736	12382.755702	28.694708
332.570278	12415.674973	28.699725
333.084501	12400.832194	28.704743
333.135898	12427.199320	28.709760
333.563152	12433.714339	28.714778
334.156701	12453.271896	28.719796
334.074013	12476.686895	28.724813
334.573173	12479.768253	28.729831
334.588853	12497.683630	28.734848
335.014922	12503.547559	28.739866
335.041732	12525.455436	28.744884
335.191508	12546.309520	28.749901
335.604575	12566.968978	28.754919
335.858020	12597.603845	28.759936
336.228800	12618.542051	28.764954
336.722603	12653.063535	28.769972
336.864054	12685.306938	28.774989
337.431183	12692.161249	28.780007
337.689542	12720.264298	28.785024
338.015503	12745.318837	28.790042
338.534613	12761.139534	28.795060
338.494430	12794.989452	28.800077
339.230318	12816.079507	28.805095
339.844233	12839.173698	28.810112
340.177148	12852.474162	28.815130
340.887208	12862.409109	28.820148
340.944223	12882.722943	28.825165
341.267053	12890.451196	28.830183
341.582362	12909.574342	28.835200
341.936829	12924.581020	28.840218
342.441594	12941.302867	28.845236
342.331728	12954.358355	28.850253
343.247308	12973.149592	28.855271
343.454466	12989.281168	28.860288
343.583672	13006.962404	28.865306
344.128987	13013.786888	28.870324
344.302554	13036.645569	28.875341
344.319323	13046.780068	28.880359
345.047288	13060.294427	28.885376
345.116598	13086.522690	28.890394
345.500451	13097.511574	28.895412
345.598743	13131.361033	28.900429
345.761422	13146.180464	28.905447
346.184016	13172.092236	28.910464
346.687332	13197.169832	28.915482
346.935060	13209.509538	28.920500
347.193600	13244.730648	28.925517
347.374351	13256.711711	28.930535
347.795709	13285.731030	28.935552
348.018150	13308.166534	28.940570
348.714316	13323.268117	28.945588
348.881450	13347.296382	28.950605
349.073819	13376.033974	28.955623
349.658803	13395.182844	28.960640
350.118433	13412.853023	28.965658
350.656493	13442.982983	28.970676
350.956193	13450.210069	28.975693
351.328098	13468.283922	28.980711
351.658192	13487.132109	28.985728
351.755438	13510.306514	28.990746
352.258713	13517.075548	28.995764
352.380482	13546.038813	29.000781
352.736657	13575.683629	29.005799
352.842541	13586.998372	29.010816
353.295775	13614.376192	29.015834
353.816687	13639.832100	29.020852
354.196259	13668.390265	29.025869
354.723094	13698.376704	29.030887
355.441690	13720.042441	29.035904
355.502853	13741.447742	29.040922
356.165574	13749.614532	29.045940
356.095789	13768.186057	29.050957
356.661421	13793.392065	29.055975
357.366984	13801.690496	29.060992
357.414728	13838.520574	29.066010
357.815462	13842.394133	29.071028
357.963345	13873.522359	29.076045
358.252422	13899.325884	29.081063
358.588224	13909.553477	29.086080
358.863422	13939.209447	29.091098
359.158660	13955.680953	29.096116
359.555105	13986.921919	29.101133
359.942139	14012.792087	29.106151
360.385608	14042.733847	29.111168
360.808547	14058.381522	29.116186
361.285576	14077.975888	29.121204
361.625410	14098.059028	29.126221
361.976620	14118.088454	29.131239
362.605455	14142.062307	29.136256
362.544845	14161.453468	29.141274
363.038996	14180.885640	29.146292
363.361424	14207.714283	29.151309
363.776496	14221.799276	29.156327
363.887132	14241.880657	29.161344
364.477345	14276.528619	29.166362
364.644846	14297.580451	29.171380
364.806703	14330.865518	29.176397
365.318503	14361.611546	29.181415
365.873200	14371.543226	29.186432
366.105142	14407.858947	29.191450
366.324386	14416.782502	29.196468
366.645863	14449.975286	29.201485
367.222706	14466.858643	29.206503
367.646379	14485.111232	29.211520
367.930484	14516.028364	29.216538
368.472866	14528.683901	29.221556
368.701948	14546.023933	29.226573
368.957472	14578.524745	29.231591
369.503171	14587.389000	29.236608
369.683438	14613.652489	29.241626
370.005256	14631.616251	29.246644
370.220901	14655.820493	29.251661
370.723794	14679.233330	29.256679
371.456152	14715.777243	29.261696
371.470325	14729.852300	29.266714
372.269363	14756.187368	29.271732
372.189254	14774.436843	29.276749
372.572254	14785.615920	29.281767
373.351273	14816.521610	29.286784
373.498726	14847.104490	29.291802
374.090052	14858.046045	29.296820
374.517410	14889.159850	29.301837
374.695642	14903.791849	29.306855
375.332095	14920.002106	29.311872
375.622223	14949.185804	29.316890
375.924058	14966.767906	29.321908
376.390186	14985.784317	29.326925
376.128846	15000.034497	29.331943
376.725443	15037.371690	29.336960
376.824049	15067.108667	29.341978
377.250968	15092.765799	29.346996
377.813536	15125.215895	29.352013
378.204273	15148.016469	29.357031
378.892369	15173.144732	29.362048
378.793889	15208.178308	29.367066
379.401895	15223.340416	29.372084
380.265380	15247.834596	29.377101
380.225864	15274.529624	29.382119
380.729512	15289.497156	29.387136
380.960096	15318.097010	29.392154
381.288548	15350.599552	29.397172
381.975766	15367.266563	29.402189
382.365599	15385.319664	29.407207
382.535186	15411.841877	29.412224
382.958427	15451.693191	29.417242
383.144850	15472.343612	29.422260
383.813296	15501.511697	29.427277
384.039430	15538.090320	29.432295
384.683201	15538.376924	29.437312
385.155636	15568.752897	29.442330
385.244775	15589.525846	29.447348
385.814404	15600.286787	29.452365
386.490019	15645.617243	29.457383
386.784879	15641.897373	29.462400
387.331587	15680.033001	29.467418
387.753107	15675.876389	29.472436
388.087831	15701.359705	29.477453
387.770787	15712.830306	29.482471
388.663140	15726.812496	29.487488
388.644003	15756.994391	29.492506
388.921172	15766.584376	29.497524
389.370878	15798.283364	29.502541
389.736986	15813.044336	29.507559
390.100972	15842.066641	29.512576
390.093986	15878.386527	29.517594
390.497964	15897.141193	29.522612
391.239974	15932.739904	29.527629
391.132945	15958.622225	29.532647
391.683868	15987.946554	29.537664
392.036696	16031.430713	29.542682
392.570494	16053.567238	29.547700
392.909135	16085.409396	29.552717
393.177364	16114.697628	29.557735
393.911955	16144.377767	29.562752
393.945047	16194.847892	29.567770
394.454911	16207.845583	29.572788
395.266760	16233.406290	29.577805
395.144759	16269.693071	29.582823
395.767291	16303.472311	29.587840
396.137887	16326.190560	29.592858
396.614978	16353.261468	29.597876
396.981899	16382.780314	29.602893
397.588376	16413.893671	29.607911
397.991347	16429.302315	29.612928
398.108785	16467.360978	29.617946
398.669387	16486.977795	29.622964
399.442638	16508.457917	29.627981
400.011392	16546.420458	29.632999
400.527656	16560.806207	29.638016
401.244788	16581.407312	29.643034
401.231213	16612.982223	29.648052
401.385887	16631.454033	29.653069
401.992542	16666.014053	29.658087
402.007250	16674.376127	29.663104
402.295723	16708.620259	29.668122
402.830525	16741.577348	29.673140
403.617648	16749.444782	29.678157
403.873960	16785.778978	29.683175
404.200190	16804.557870	29.688192
404.320573	16836.937183	29.693210
404.989641	16857.972053	29.698228
405.459016	16880.828120	29.703245
405.581525	16911.215563	29.708263
406.334732	16928.759784	29.713280
406.639969	16968.309856	29.718298
406.870196	16982.796690	29.723316
407.310534	17012.831955	29.728333
408.042419	17034.464076	29.733351
408.215095	17069.865129	29.738368
408.692358	17084.471539	29.743386
409.133112	17108.976619	29.748404
409.732403	17132.655380	29.753421
409.844580	17154.153366	29.758439
410.265956	17166.285945	29.763456
410.817843	17188.142022	29.768474
410.832032	17220.616414	29.773492
411.525400	17238.031365	29.778509
411.943686	17265.903330	29.783527
412.091781	17282.088016	29.788544
412.440661	17303.410515	29.793562
412.977894	17330.297200	29.798580
413.059526	17350.203032	29.803597
413.119323	17388.460535	29.808615
413.923126	17419.029768	29.813632
414.234205	17439.937452	29.818650
414.428942	17487.349691	29.823668
414.986410	17513.053646	29.828685
415.524337	17545.043728	29.833703
415.639156	17579.734555	29.838720
416.358349	17616.987825	29.843738
416.664716	17646.271514	29.848756
417.177834	17679.031716	29.853773
417.494628	17717.072717	29.858791
418.261210	17741.469411	29.863808
418.649082	17765.124567	29.868826
419.028947	17794.774952	29.873844
419.851503	17822.770113	29.878861
420.238649	17842.621404	29.883879
420.523339	17871.616865	29.888896
420.942855	17898.898866	29.893914
421.306819	17924.415453	29.898932
421.621819	17950.460329	29.903949
422.020944	17985.317778	29.908967
422.931896	18010.775307	29.913984
423.189545	18039.008104	29.919002
423.421475	18069.379207	29.924020
423.911766	18103.620062	29.929037
424.371773	18127.275303	29.934055
424.497298	18145.758883	29.939072
425.132148	18177.059661	29.944090
425.555259	18214.880623	29.949108
426.237155	18237.523943	29.954125
426.201041	18271.328979	29.959143
426.945754	18289.653842	29.964160
427.347438	18320.661362	29.969178
427.883598	18346.817333	29.974196
428.723218	18365.007877	29.979213
428.890793	18392.223806	29.984231
429.294373	18414.230248	29.989248
429.672405	18438.114375	29.994266
429.893043	18469.651423	29.999284
430.163611	18488.155608	30.004301
430.467287	18517.886642	30.009319
431.245111	18551.153950	30.014336
431.613449	18572.544588	30.019354
432.027568	18604.380606	30.024372
432.591416	18618.083151	30.029389
432.908267	18642.593477	30.034407
433.218563	18669.671799	30.039424
433.714364	18690.713160	30.044442
433.915921	18713.110875	30.049460
434.588426	18731.634383	30.054477
434.587430	18776.077029	30.059495
435.588893	18788.546615	30.064512
435.777494	18820.755623	30.069530
435.825145	18849.198944	30.074548
436.868574	18869.313923	30.079565
436.898353	18913.786705	30.084583
437.328301	18938.856257	30.089600
437.734655	18972.662007	30.094618
437.881614	18991.844370	30.099636
438.489168	19022.859865	30.104653
438.748670	19069.211089	30.109671
439.546003	19096.327522	30.114688
439.955720	19132.417384	30.119706
440.216622	19172.968558	30.124724
440.769459	19202.182058	30.129741
441.235038	19237.136460	30.134759
441.877735	19272.641087	30.139776
442.226171	19293.538236	30.144794
442.467753	19332.671989	30.149812
443.228522	19364.881125	30.154829
443.758737	19400.148836	30.159847
443.995073	19430.044318	30.164864
444.577528	19462.297814	30.169882
444.878911	19494.330003	30.174900
445.797875	19507.899986	30.179917
445.785680	19534.932371	30.184935
446.281614	19566.901429	30.189952
447.480887	19590.470653	30.194970
447.499457	19618.778665	30.199988
448.160477	19648.675415	30.205005
448.521757	19667.329554	30.210023
448.717975	19694.171128	30.215040
449.582650	19722.500837	30.220058
449.636112	19747.062348	30.225076
450.218530	19774.500447	30.230093
450.614155	19804.981153	30.235111
450.697098	19833.995095	30.240128
451.377473	19867.746534	30.245146
451.553731	19896.592959	30.250164
452.499519	19918.714379	30.255181
452.707593	19966.899041	30.260199
453.085278	19995.101698	30.265216
453.783435	20015.439336	30.270234
453.831778	20064.952608	30.275252
454.691178	20080.452825	30.280269
455.128506	20114.083270	30.285287
455.629386	20128.790580	30.290304
455.793340	20162.782427	30.295322
456.195292	20193.528262	30.300340
456.552106	20207.932585	30.305357
456.806166	20250.311046	30.310375
457.560446	20272.837139	30.315392
458.020308	20306.725458	30.320410
458.086676	20338.757055	30.325428
458.255925	20369.643076	30.330445
458.812739	20400.322123	30.335463
459.509543	20448.547742	30.340480
459.676174	20468.666683	30.345498
460.086657	20517.209811	30.350516
460.672806	20545.209366	30.355533
461.569889	20587.194925	30.360551
461.812078	20629.154600	30.365568
462.653163	20646.697522	30.370586
462.523445	20687.229808	30.375604
463.279101	20710.180384	30.380621
463.769981	20743.772940	30.385639
464.020630	20776.605706	30.390656
464.867294	20815.193173	30.395674
465.196582	20855.376748	30.400692
465.350935	20883.057458	30.405709
465.552058	20923.389202	30.410727
466.391859	20966.249985	30.415744
467.352350	20988.371375	30.420762
467.784717	21036.956729	30.425780
468.120065	21066.741522	30.430797
468.722087	21098.996468	30.435815
468.993450	21127.481138	30.440832
469.878780	21159.118153	30.445850
469.926572	21194.743589	30.450868
470.955217	21206.984793	30.455885
471.046656	21246.485889	30.460903
471.506505	21281.700154	30.465920
471.947646	21304.732030	30.470938
472.270731	21337.148852	30.475956
472.609052	21387.013472	30.480973
473.236498	21413.942472	30.485991
473.771280	21452.313435	30.491008
474.436955	21490.107637	30.496026
474.577136	21540.509121	30.501044
474.986793	21569.502578	30.506061
475.549831	21598.236177	30.511079
476.416312	21627.798027	30.516096
477.000703	21662.262463	30.521114
476.979302	21699.560215	30.526132
477.580625	21732.941591	30.531149
478.241211	21773.565382	30.536167
478.400978	21804.123783	30.541184
479.155726	21821.225792	30.546202
479.148817	21862.359377	30.551220
479.645873	21894.062883	30.556237
480.486963	21936.344504	30.561255
480.817974	21978.896512	30.566272
481.614705	22008.563912	30.571290
482.060332	22040.820902	30.576308
482.325310	22067.971795	30.581325
482.936850	22090.824105	30.586343
483.283943	22120.074266	30.591360
483.727288	22158.255964	30.596378
484.080835	22191.243046	30.601396
484.688353	22211.604290	30.606413
485.165827	22249.672875	30.611431
485.231516	22283.988971	30.616448
486.166954	22304.981715	30.621466
486.753223	22351.413062	30.626484
487.168880	22379.974676	30.631501
487.231123	22409.688171	30.636519
487.789428	22445.678519	30.641536
488.005142	22481.158037	30.646554
488.599764	22535.829133	30.651572
489.058593	22573.918011	30.656589
489.624139	22591.579478	30.661607
489.941085	22653.024416	30.666624
490.793445	22686.936472	30.671642
491.162555	22727.084618	30.676660
491.723156	22762.079796	30.681677
492.319373	22798.391765	30.686695
492.843303	22848.420467	30.691712
493.403784	22873.781913	30.696730
493.741587	22919.610250	30.701748
494.553460	22947.344217	30.706765
495.233075	22975.243435	30.711783
495.489666	23016.374279	30.716800
496.033371	23046.288726	30.721818
496.749587	23081.394506	30.726836
497.038687	23126.096242	30.731853
497.457262	23156.433306	30.736871
497.705979	23191.074280	30.741888
498.523172	23226.756591	30.746906
498.578238	23277.182690	30.751924
499.110382	23317.263832	30.756941
499.879466	23359.515851	30.761959
500.321537	23404.635079	30.766976
500.752597	23440.641665	30.771994
501.239106	23483.543934	30.777012
501.818989	23513.963106	30.782029
501.877199	23555.943734	30.787047
502.695507	23599.806369	30.792064
503.496642	23625.470951	30.797082
503.844696	23674.240118	30.802100
504.496393	23713.805427	30.807117
505.120594	23745.895679	30.812135
505.426853	23785.515406	30.817152
505.960388	23814.936708	30.822170
506.779919	23848.386263	30.827188
507.181137	23892.787958	30.832205
507.621948	23930.027576	30.837223
507.941436	23958.214320	30.842240
508.857953	23984.790547	30.847258
509.427629	24023.357548	30.852276
509.539109	24055.890853	30.857293
510.198735	24079.801740	30.862311
510.643588	24109.707166	30.867328
511.209485	24136.812890	30.872346
511.416382	24170.976674	30.877364
511.847649	24193.216436	30.882381
512.436182	24233.947835	30.887399
512.667852	24283.409299	30.892416
513.623979	24323.738947	30.897434
513.665417	24362.885580	30.902452
513.725166	24395.174973	30.907469
514.538800	24448.696916	30.912487
515.022460	24493.542440	30.917504
515.447962	24534.364381	30.922522
516.321533	24568.349568	30.927540
516.571381	24607.481721	30.932557
517.452227	24662.399711	30.937575
517.638811	24707.699611	30.942592
518.423314	24741.509522	30.947610
518.959975	24787.165064	30.952628
519.466437	24825.749597	30.957645
520.066158	24859.415110	30.962663
520.388350	24913.041317	30.967680
520.839359	24958.249395	30.972698
521.507535	24995.100035	30.977716
521.751466	25046.900636	30.982733
522.562159	25087.757165	30.987751
523.012557	25141.275492	30.992768
523.421662	25177.496683	30.997786
524.266113	25222.512079	31.002804
524.718822	25259.022694	31.007821
525.818216	25302.360813	31.012839
526.226499	25337.385153	31.017856
526.391319	25366.534063	31.022874
527.096562	25412.391410	31.027892
527.705869	25452.478254	31.032909
528.085880	25487.342001	31.037927
528.364701	25534.220784	31.042944
529.218080	25569.448868	31.047962
529.746540	25614.087172	31.052980
530.312498	25646.149580	31.057997
531.173914	25693.794673	31.063015
531.385127	25732.532413	31.068032
531.911690	25771.459492	31.073050
532.327826	25809.359694	31.078068
532.877552	25857.433045	31.083085
533.751997	25880.449837	31.088103
534.258901	25927.059477	31.093120
534.661545	25954.695319	31.098138
535.375839	26002.886266	31.103156
535.542014	26042.291286	31.108173
536.132904	26066.109766	31.113191
536.392506	26115.104522	31.118208
537.456494	26159.406176	31.123226
537.668868	26186.572491	31.128244
538.018997	26228.664904	31.133261
538.578418	26254.715714	31.138279
538.698655	26308.433911	31.143296
539.473444	26351.019903	31.148314
540.233160	26378.356178	31.153332
540.698689	26425.025063	31.158349
541.588626	26444.314778	31.163367
541.886606	26481.876164	31.168384
542.343737	26522.846255	31.173402
542.798235	26569.036767	31.178420
543.147248	26609.157730	31.183437
543.746572	26638.685639	31.188455
543.984014	26697.934901	31.193472
544.533785	26749.706476	31.198490
545.146195	26797.513478	31.203508
545.535895	26839.900556	31.208525
546.205449	26885.928526	31.213543
546.765586	26942.901742	31.218560
547.605122	26991.922611	31.223578
547.992270	27032.044071	31.228596
548.433570	27089.662258	31.233613
549.026348	27125.460756	31.238631
549.567532	27171.845602	31.243648
550.235919	27228.277111	31.248666
551.111663	27266.716541	31.253684
551.512655	27325.205447	31.258701
552.042200	27358.517912	31.263719
552.662567	27406.616168	31.268736
553.420907	27449.679609	31.273754
554.215012	27488.948769	31.278772
554.322235	27539.063287	31.283789
554.903211	27582.955777	31.288807
555.093723	27632.232450	31.293824
555.576803	27689.267852	31.298842
556.629497	27732.498673	31.303860
557.202195	27774.201213	31.308877
557.649449	27815.476341	31.313895
558.397920	27872.310975	31.318912
558.919897	27903.615959	31.323930
559.640138	27951.615635	31.328948
560.050963	28002.625513	31.333965
560.797580	28031.566053	31.338983
561.431438	28083.872151	31.344000
561.815184	28124.300989	31.349018
562.554915	28158.773675	31.354036
563.069871	28204.430590	31.359053
563.428139	28247.826186	31.364071
563.890972	28296.260246	31.369088
564.022544	28345.141149	31.374106
565.278710	28377.630116	31.379124
565.678963	28439.772632	31.384141
566.398978	28472.195909	31.389159
567.035226	28518.467853	31.394176
567.359837	28569.858831	31.399194
567.913131	28598.019655	31.404212
568.380780	28642.870667	31.409229
569.040897	28683.721742	31.414247
569.570238	28719.916804	31.419264
569.952745	28765.949377	31.424282
570.789482	28807.160280	31.429300
571.029182	28840.951376	31.434317
571.945246	28881.210656	31.439335
572.277427	28924.839138	31.444352
572.510562	28968.582789	31.449370
573.249213	29004.789274	31.454388
573.760486	29065.930049	31.459405
574.032752	29108.159780	31.464423
574.547466	29170.236441	31.469440
575.442749	29212.520074	31.474458
575.875190	29271.427033	31.479476
576.387571	29311.237951	31.484493
577.076589	29368.596313	31.489511
577.650914	29414.127421	31.494528
577.969646	29480.617365	31.499546
578.929164	29514.118724	31.504564
579.320951	29568.263085	31.509581
579.874077	29621.345004	31.514599
580.390744	29682.960005	31.519616
580.814840	29736.100669	31.524634
581.884851	29793.984510	31.529652
582.317341	29840.560581	31.534669
582.985370	29906.415128	31.539687
583.640436	29959.957840	31.544704
584.212588	30006.368734	31.549722
585.044154	30064.168592	31.554740
585.568039	30103.818877	31.559757
586.028932	30156.551616	31.564775
586.683831	30201.766367	31.569792
587.114783	30250.699877	31.574810
588.214947	30298.630244	31.579828
588.382612	30365.403161	31.584845
589.232180	30399.656678	31.589863
589.943445	30459.070386	31.594880
590.294498	30508.605227	31.599898
591.147403	30550.117418	31.604916
591.538333	30605.623846	31.609933
592.017621	30647.731618	31.614951
592.755436	30702.595293	31.619968
593.232680	30762.559570	31.624986
593.910630	30802.412384	31.630004
594.696376	30846.139261	31.635021
595.184809	30894.080549	31.640039
596.039900	30945.854741	31.645056
596.532861	30993.091124	31.650074
597.150357	31024.987383	31.655092
597.625741	31090.256442	31.660109
598.159887	31137.800312	31.665127
598.840940	31171.763936	31.670144
599.392587	31216.159498	31.675162
600.521644	31257.361587	31.680180
600.776207	31308.067875	31.685197
601.046560	31334.852190	31.690215
601.907732	31367.638601	31.695232
601.983324	31419.040402	31.700250
602.514033	31460.757524	31.705268
603.287663	31514.317977	31.710285
603.657531	31557.537728	31.715303
603.874197	31606.660726	31.720320
604.863916	31661.096637	31.725338
605.562829	31720.923527	31.730356
605.719500	31773.659497	31.735373
606.387668	31824.750699	31.740391
607.022944	31874.044246	31.745408
607.554167	31929.769235	31.750426
608.636484	31982.886460	31.755444
609.351406	32046.768883	31.760461
609.582672	32091.000333	31.765479
610.247169	32141.538314	31.770496
610.912443	32206.887177	31.775514
611.609610	32258.347076	31.780532
611.865757	32316.528665	31.785549
613.013866	32375.759977	31.790567
613.290021	32430.682473	31.795584
614.193549	32499.017607	31.800602
614.711442	32550.398215	31.805620
615.123868	32585.750439	31.810637
615.640670	32653.544130	31.815655
616.526430	32716.859749	31.820672
617.154235	32762.798324	31.825690
618.009728	32812.967499	31.830708
618.396091	32870.611743	31.835725
619.062675	32922.978596	31.840743
620.150754	32979.816374	31.845760
620.391223	33042.107446	31.850778
621.210432	33090.724378	31.855796
621.572921	33142.749456	31.860813
622.216181	33203.430725	31.865831
622.807027	33246.389596	31.870848
623.341989	33305.165491	31.875866
624.284145	33363.046074	31.880884
624.807264	33417.640924	31.885901
625.073157	33483.236565	31.890919
625.957656	33542.417906	31.895936
626.486457	33601.942982	31.900954
627.281015	33652.310415	31.905972
627.984227	33713.199958	31.910989
628.387839	33766.894451	31.916007
629.341965	33812.845461	31.921024
629.652916	33865.525719	31.926042
630.455704	33915.752355	31.931060
631.150512	33980.794592	31.936077
631.582172	34037.510407	31.941095
632.348278	34083.075967	31.946112
632.643141	34150.307416	31.951130
633.608865	34207.020734	31.956148
634.329180	34254.350075	31.961165
634.838855	34290.029371	31.966183
635.367575	34352.195925	31.971200
636.113759	34404.617853	31.976218
636.800079	34445.677763	31.981236
637.099348	34487.803540	31.986253
637.780579	34541.502048	31.991271
638.989036	34593.291358	31.996288
639.228126	34641.749863	32.001306
639.797672	34697.429226	32.006324
640.608606	34752.632107	32.011341
640.719072	34811.506166	32.016359
641.509355	34872.181175	32.021376
641.691386	34921.012147	32.026394
642.867347	34983.971810	32.031412
643.632815	35033.072776	32.036429
644.186657	35086.752346	32.041447
644.827633	35141.239522	32.046464
645.271137	35212.061565	32.051482
646.416898	35265.486663	32.056500
647.118167	35313.501494	32.061517
647.626150	35372.733564	32.066535
648.413477	35425.656622	32.071552
649.142074	35486.398871	32.076570
649.809042	35528.602730	32.081588
650.095169	35593.151992	32.086605
650.756548	35638.911911	32.091623
651.709954	35692.365859	32.096640
651.993402	35764.670805	32.101658
652.739350	35815.145558	32.106676
653.604046	35866.508028	32.111693
654.177276	35931.471635	32.116711
654.915583	35983.704314	32.121728
655.322827	36049.256038	32.126746
655.984264	36113.421215	32.131764
656.697749	36170.071045	32.136781
657.485913	36225.504724	32.141799
658.353167	36282.882446	32.146816
659.114849	36337.866679	32.151834
659.568729	36385.671748	32.156852
660.248703	36442.696744	32.161869
660.729602	36491.391704	32.166887
661.840120	36555.381443	32.171904
662.050012	36621.091377	32.176922
662.911929	36659.544835	32.181940
663.460684	36727.217633	32.186957
664.004223	36790.496084	32.191975
664.927049	36841.239015	32.196992
665.023884	36908.508381	32.202010
665.747032	36961.668823	32.207028
666.806285	37020.986074	32.212045
667.240999	37081.884971	32.217063
668.323442	37136.838098	32.222080
668.885198	37199.612258	32.227098
669.621224	37235.755297	32.232116
669.911359	37300.458700	32.237133
670.614561	37340.829349	32.242151
671.587881	37388.948723	32.247168
672.211315	37441.943679	32.252186
672.397347	37500.782054	32.257204
673.502465	37543.591304	32.262221
673.922629	37601.968640	32.267239
675.074256	37650.599585	32.272256
674.859979	37708.277373	32.277274
675.469694	37759.941673	32.282292
676.225703	37816.303346	32.287309
676.868403	37893.041121	32.292327
677.852685	37940.617960	32.297344
678.478173	38006.543052	32.302362
679.056845	38068.363873	32.307380
679.402349	38136.557172	32.312397
680.349601	38178.760927	32.317415
681.356656	38248.465454	32.322432
681.813821	38319.716273	32.327450
682.693745	38379.074758	32.332468
683.567831	38448.517476	32.337485
683.797746	38514.712510	32.342503
684.735151	38566.965681	32.347520
685.226018	38630.232633	32.352538
685.762756	38696.587655	32.357556
686.664260	38768.811845	32.362573
687.052080	38829.517970	32.367591
687.895526	38887.611614	32.372608
688.355218	38971.067299	32.377626
688.782792	39031.834044	32.382644
690.334002	39100.241336	32.387661
690.825534	39173.609468	32.392679
691.802044	39226.981125	32.397696
692.376056	39295.961069	32.402714
693.259633	39353.591077	32.407732
693.958261	39415.859731	32.412749
694.631492	39478.474825	32.417767
695.890804	39520.495072	32.422784
696.436385	39593.211497	32.427802
697.185177	39642.251349	32.432820
698.081337	39687.019897	32.437837
698.631452	39765.185865	32.442855
699.322072	39807.644275	32.447872
699.745987	39871.554104	32.452890
700.298799	39923.498989	32.457908
701.059914	39980.972445	32.462925
701.744532	40054.693666	32.467943
702.561341	40096.699072	32.472960
702.964744	40153.563048	32.477978
703.745937	40222.475925	32.482996
704.767784	40276.214239	32.488013
705.276385	40332.426579	32.493031
706.139271	40389.557222	32.498048
706.555611	40455.138805	32.503066
706.946649	40519.683909	32.508084
707.763534	40564.087358	32.513101
707.912379	40631.377426	32.518119
709.141666	40682.179313	32.523136
709.829543	40743.650314	32.528154
710.385315	40798.563602	32.533172
711.170762	40850.029582	32.538189
711.377167	40922.401989	32.543207
712.634457	40984.970644	32.548224
713.308350	41052.893139	32.553242
714.014344	41114.023545	32.558260
715.187228	41170.389935	32.563277
715.237580	41242.954125	32.568295
716.256523	41300.007781	32.573312
716.959510	41357.105623	32.578330
717.349363	41418.577615	32.583348
718.266983	41479.047993	32.588365
718.953403	41545.267295	32.593383
719.767059	41606.991047	32.598400
720.641051	41672.061302	32.603418
721.011565	41737.010101	32.608436
722.020906	41803.762490	32.613453
722.292532	41877.029030	32.618471
723.432459	41928.072800	32.623488
724.453533	42002.920610	32.628506
724.633551	42067.320636	32.633524
725.836601	42126.129806	32.638541
726.325591	42202.346920	32.643559
727.171222	42257.542043	32.648576
727.817403	42335.579891	32.653594
728.313718	42408.096934	32.658612
729.150929	42466.224286	32.663629
730.115271	42532.340072	32.668647
730.881950	42606.281605	32.673664
731.450991	42667.082933	32.678682
731.842169	42741.390785	32.683700
733.102881	42807.706478	32.688717
733.726273	42869.862499	32.693735
734.889816	42932.052616	32.698752
735.603252	43007.944221	32.703770
736.148371	43071.794661	32.708788
737.042336	43127.704062	32.713805
737.431620	43196.295443	32.718823
738.329295	43253.983693	32.723840
739.302967	43314.688194	32.728858
739.966603	43389.766129	32.733876
740.908904	43445.097931	32.738893
741.395679	43511.230420	32.743911
742.099466	43569.799119	32.748928
742.679535	43631.204579	32.753946
743.376195	43709.199608	32.758964
744.315074	43768.526464	32.763981
744.760086	43842.568671	32.768999
745.635732	43907.867937	32.774016
746.502909	43972.468511	32.779034
746.940703	44034.074700	32.784052
747.929534	44087.918561	32.789069
748.541117	44148.390272	32.794087
749.368836	44196.493730	32.799104
749.876435	44264.360753	32.804122
750.987734	44330.854358	32.809140
751.581982	44379.459206	32.814157
752.193222	44450.326181	32.819175
753.159986	44513.048590	32.824192
753.761648	44562.744245	32.829210
754.155158	44631.173449	32.834228
755.304674	44690.290127	32.839245
755.605888	44761.936437	32.844263
756.797157	44820.589498	32.849280
757.560398	44901.229162	32.854298
757.963605	44967.295338	32.859316
759.026891	45037.714196	32.864333
759.219857	45102.281196	32.869351
760.200859	45173.060713	32.874368
761.383452	45247.388990	32.879386
761.648100	45315.374506	32.884404
762.820710	45377.767579	32.889421
763.704782	45446.500464	32.894439
764.426166	45524.152700	32.899456
765.150458	45596.173602	32.904474
765.674994	45655.717997	32.909492
766.577194	45735.178457	32.914509
767.210399	45809.814270	32.919527
768.091675	45880.369622	32.924544
769.074610	45942.173418	32.929562
769.487591	46025.498844	32.934580
770.459340	46090.724773	32.939597
770.947302	46160.170268	32.944615
771.803506	46228.128270	32.949632
772.791974	46311.139455	32.954650
773.172907	46402.418902	32.959668
774.448921	46457.271821	32.964685
775.136020	46540.186940	32.969703
775.778214	46609.890456	32.974720
776.880438	46673.255316	32.979738
777.709265	46754.442069	32.984756
778.405536	46822.257472	32.989773
779.276614	46894.847186	32.994791
779.758357	46976.232190	32.999808
780.833844	47045.688634	33.004826
781.244748	47127.303310	33.009844
782.354617	47185.314741	33.014861
783.196450	47272.707767	33.019879
783.456643	47332.751119	33.024896
784.722387	47402.093506	33.029914
785.329275	47481.047301	33.034932
786.006734	47558.964811	33.039949
786.904208	47627.347612	33.044967
787.603641	47707.691717	33.049984
788.636841	47766.218940	33.055002
789.556603	47831.642629	33.060020
790.533743	47886.481347	33.065037
791.037751	47951.441593	33.070055
791.751821	48013.339673	33.075072
792.702883	48064.620903	33.080090
793.338919	48130.254935	33.085108
793.891505	48194.277561	33.090125
794.814713	48273.011022	33.095143
795.582024	48338.003352	33.100160
796.091726	48402.989598	33.105178
796.771434	48470.205033	33.110196
797.870509	48538.625546	33.115213
798.666046	48611.366894	33.120231
799.560561	48690.532749	33.125248
800.344693	48746.092722	33.130266
801.123778	48815.464505	33.135284
801.921919	48901.531557	33.140301
802.416997	48975.171012	33.145319
803.333226	49039.949747	33.150336
804.005554	49113.482680	33.155354
804.639820	49201.593558	33.160372
805.774211	49267.102004	33.165389
806.108634	49347.748327	33.170407
806.889439	49441.661970	33.175424
807.979396	49510.491593	33.180442
808.864782	49607.289321	33.185460
809.646583	49671.397562	33.190477
810.471083	49764.409804	33.195495
811.460801	49832.461450	33.200512
811.895461	49913.965307	33.205530
812.919376	49986.868440	33.210548
813.830217	50069.783473	33.215565
814.843696	50143.746019	33.220583
815.457269	50230.047693	33.225600
816.668764	50304.500060	33.230618
817.420872	50386.580361	33.235636
818.368443	50445.915836	33.240653
819.524767	50525.183903	33.245671
820.389760	50596.357150	33.250688
821.600591	50653.414071	33.255706
822.151212	50726.771092	33.260724
823.001194	50791.159685	33.265741
823.618789	50856.652117	33.270759
824.116148	50931.902401	33.275776
825.262493	51005.433986	33.280794
826.236478	51080.261907	33.285812
826.851105	51146.582675	33.290829
827.522710	51214.024377	33.295847
828.348277	51280.974777	33.300864
829.632959	51354.346929	33.305882
830.427087	51432.004118	33.310900
830.804089	51498.749018	33.315917
831.460312	51571.054441	33.320935
832.160566	51656.711741	33.325952
833.640159	51718.112735	33.330970
834.398564	51788.351481	33.335988
834.890753	51850.566498	33.341005
835.542193	51911.677079	33.346023
836.256199	51983.924477	33.351040
837.136547	52039.403686	33.356058
837.764875	52124.465582	33.361076
838.463093	52191.092505	33.366093
839.393260	52269.653201	33.371111
839.865161	52354.015216	33.376128
840.795186	52424.184953	33.381146
841.229622	52519.747893	33.386164
842.229690	52586.044202	33.391181
843.175355	52674.425632	33.396199
844.032324	52760.476692	33.401216
845.046383	52838.868724	33.406234
845.689923	52936.669782	33.411252
846.203924	53011.484291	33.416269
847.435090	53108.327998	33.421287
848.292152	53184.429958	33.426304
849.366526	53279.891925	33.431322
850.210823	53366.733767	33.436340
851.116924	53451.098091	33.441357
851.987191	53535.566353	33.446375
852.529658	53621.494830	33.451392
853.679036	53714.242321	33.456410
854.315461	53795.794827	33.461428
855.583576	53872.506540	33.466445
856.875461	53952.642455	33.471463
857.346397	54038.577984	33.476480
858.471506	54116.424488	33.481498
859.679721	54200.185570	33.486516
860.418807	54267.915200	33.491533
861.002433	54346.978818	33.496551
862.044594	54439.677653	33.501568
863.022648	54502.629353	33.506586
863.772426	54592.380152	33.511604
864.716735	54667.057272	33.516621
865.675409	54734.763168	33.521639
866.378315	54824.102775	33.526656
867.646432	54897.302629	33.531674
868.307116	54976.710241	33.536692
869.140843	55055.127954	33.541709
869.950310	55133.351010	33.546727
870.414754	55214.419607	33.551744
871.575721	55284.936159	33.556762
872.087147	55377.377029	33.561780
872.807179	55458.074605	33.566797
874.070492	55552.208529	33.571815
874.370797	55635.580956	33.576832
875.468535	55718.173457	33.581850
876.506160	55811.773305	33.586868
877.316187	55899.080945	33.591885
878.488166	55980.119260	33.596903
879.136205	56073.848737	33.601920
880.435105	56143.734284	33.606938
880.942622	56216.283958	33.611956
881.974463	56297.772127	33.616973
882.716928	56359.356727	33.621991
883.771278	56428.944523	33.627008
884.631128	56507.373790	33.632026
885.386037	56588.326496	33.637044
886.134358	56662.017057	33.642061
887.109617	56733.190629	33.647079
887.663523	56834.076288	33.652096
888.876145	56894.347278	33.657114
889.624498	56980.344061	33.662132
890.144130	57065.405362	33.667149
891.101580	57143.894425	33.672167
891.975999	57239.762542	33.677184
892.564493	57319.084481	33.682202
893.388193	57414.181847	33.687220
894.255578	57498.552133	33.692237
895.328883	57593.790647	33.697255
896.222877	57698.247836	33.702272
897.293572	57787.609676	33.707290
898.069121	57884.238751	33.712308
899.184892	57974.339352	33.717325
900.241498	58064.137273	33.722343
901.097447	58157.282357	33.727360
901.779625	58248.772901	33.732378
902.988414	58337.244108	33.737396
904.004908	58444.735672	33.742413
905.008107	58524.321973	33.747431
905.331730	58611.931419	33.752448
906.480888	58698.377562	33.757466
907.606226	58796.281702	33.762484
908.255828	58898.981889	33.767501
909.637307	58976.082149	33.772519
910.246383	59072.418742	33.777536
911.536920	59160.400999	33.782554
912.326860	59260.018448	33.787572
913.128324	59348.344619	33.792589
914.099592	59433.288123	33.797607
915.056241	59524.371902	33.802624
916.062581	59617.825590	33.807642
916.879807	59702.027635	33.812660
917.720432	59800.086566	33.817677
918.565862	59892.105439	33.822695
919.341292	59995.290507	33.827712
920.126470	60083.714323	33.832730
921.189664	60177.366996	33.837748
922.130928	60269.662957	33.842765
923.351320	60370.442891	33.847783
924.170293	60469.329691	33.852800
925.094676	60546.562881	33.857818
926.124867	60652.075902	33.862836
926.722666	60747.141058	33.867853
928.184262	60828.893408	33.872871
928.860625	60922.036724	33.877888
929.755252	61012.360917	33.882906
930.997880	61103.602668	33.887924
931.693336	61185.099589	33.892941
932.586079	61264.749924	33.897959
933.193982	61347.022432	33.902976
934.157316	61425.127678	33.907994
935.169199	61504.261189	33.913012
935.809132	61595.342317	33.918029
936.913279	61683.242999	33.923047
937.756818	61769.088939	33.928064
938.754908	61860.537478	33.933082
939.616759	61958.721180	33.938100
940.435195	62047.499473	33.943117
941.686938	62135.574560	33.948135
942.485042	62233.605643	33.953152
943.330197	62326.924845	33.958170
944.188355	62409.181129	33.963188
945.130647	62518.684665	33.968205
946.017130	62612.901805	33.973223
946.858796	62724.490841	33.978240
948.171585	62818.180150	33.983258
949.245801	62925.094658	33.988276
949.530672	63017.375945	33.993293
950.714222	63117.687042	33.998311
951.562171	63232.135871	34.003328
952.676718	63337.783174	34.008346
953.699460	63440.148888	34.013364
954.637390	63541.581294	34.018381
955.733434	63638.937535	34.023399
956.739261	63729.370752	34.028416
957.603783	63838.499567	34.033434
958.728606	63945.307574	34.038452
959.593641	64054.914398	34.043469
960.989441	64153.728769	34.048487
961.739349	64256.555992	34.053504
962.663419	64353.191661	34.058522
963.909057	64443.466963	34.063540
964.632018	64550.162301	34.068557
965.732045	64656.416121	34.073575
966.739107	64759.899918	34.078592
967.550881	64844.258472	34.083610
968.767547	64943.364410	34.088628
969.528421	65051.847159	34.093645
970.632794	65146.035897	34.098663
971.687362	65244.802849	34.103680
972.632590	65344.023533	34.108698
973.940780	65445.719839	34.113716
974.706592	65544.303733	34.118733
976.064722	65630.170563	34.123751
976.686981	65720.011035	34.128768
977.857345	65814.808423	34.133786
979.066706	65910.342265	34.138804
979.607684	66010.530820	34.143821
980.909221	66108.239661	34.148839
981.984772	66196.314253	34.153856
982.508006	66282.714783	34.158874
983.858509	66355.605436	34.163892
984.570441	66442.819938	34.168909
985.189459	66533.940704	34.173927
986.389508	66614.098374	34.178944
987.433608	66706.737830	34.183962
988.086914	66790.324783	34.188980
988.934988	66895.743610	34.193997
990.031043	66969.507738	34.199015
990.916942	67066.965422	34.204032
991.362665	67173.444686	34.209050
992.509788	67270.991340	34.214068
993.335552	67370.181489	34.219085
994.613725	67474.530656	34.224103
995.359344	67590.348425	34.229120
996.377512	67689.098994	34.234138
997.729194	67788.182354	34.239156
997.997188	67911.165826	34.244173
999.324318	68011.094414	34.249191
1000.306542	68119.341309	34.254208
1001.089248	68235.138081	34.259226
1002.463733	68350.317065	34.264244
1003.834045	68450.260003	34.269261
1004.635807	68561.886259	34.274279
1005.707252	68677.469168	34.279296
1006.650195	68773.160656	34.284314
1007.713642	68879.920593	34.289332
1008.416049	69002.753419	34.294349
1009.884775	69095.526291	34.299367
1011.249489	69206.542335	34.304384
1012.061280	69328.336367	34.309402
1013.260545	69417.483110	34.314420
1013.827524	69530.327350	34.319437
1015.127014	69640.326461	34.324455
1016.420265	69749.316345	34.329472
1017.513376	69847.648994	34.334490
1018.741800	69956.220737	34.339508
1019.302379	70054.133715	34.344525
1020.665349	70150.068401	34.349543
1021.618550	70242.113734	34.354560
1022.649561	70355.046861	34.359578
1024.099766	70459.485775	34.364596
1024.798101	70560.885847	34.369613
1026.023353	70649.705544	34.374631
1027.169666	70758.844470	34.379648
1028.024802	70858.306760	34.384666
1029.012056	70949.421237	34.389684
1029.757692	71065.550280	34.394701
1031.279194	71168.180949	34.399719
1032.333944	71258.224662	34.404736
1032.937586	71365.008125	34.409754
1034.309100	71454.395795	34.414772
1034.950366	71559.702165	34.419789
1035.862571	71666.539270	34.424807
1036.993760	71774.062417	34.429824
1037.561761	71878.137416	34.434842
1038.772451	71968.241709	34.439860
1039.833242	72070.204788	34.444877
1040.864836	72163.371336	34.449895
1042.049648	72261.891039	34.454912
1042.697926	72360.957836	34.459930
1044.070027	72458.873737	34.464948
1045.050857	72549.434273	34.469965
1046.144417	72656.115188	34.474983
1046.972983	72755.945117	34.480000
1047.758287	72855.327479	34.485018
1049.214885	72946.212231	34.490036
1050.174801	73058.654014	34.495053
1050.990435	73166.399210	34.500071
1052.111452	73271.044398	34.505088
1052.887771	73385.324430	34.510106
1054.214038	73488.699609	34.515124
1055.059112	73596.916374	34.520141
1056.254394	73708.161699	34.525159
1057.130852	73828.690487	34.530176
1058.354114	73937.057472	34.535194
1059.698134	74044.470608	34.540212
1060.533603	74168.534037	34.545229
1061.670086	74289.365481	34.550247
1062.632958	74389.460282	34.555264
1063.339043	74511.549543	34.560282
1064.758837	74619.610923	34.565300
1065.413091	74741.280116	34.570317
1066.505008	74868.624746	34.575335
1067.876695	74981.763874	34.580352
1069.167584	75099.504414	34.585370
1070.453843	75205.770196	34.590388
1071.585390	75330.520467	34.595405
1072.737505	75442.016124	34.600423
1073.960550	75556.502925	34.605440
1074.579341	75680.155158	34.610458
1075.794665	75779.837564	34.615476
1076.959964	75899.802013	34.620493
1078.160853	75999.178136	34.625511
1079.456091	76122.219911	34.630528
1080.352262	76239.676000	34.635546
1081.860298	76335.895587	34.640564
1082.616477	76453.223509	34.645581
1083.424687	76570.708153	34.650599
1084.971981	76663.655665	34.655616
1085.951574	76791.150398	34.660634
1087.007848	76895.034799	34.665652
1088.206673	77007.561843	34.670669
1089.134971	77120.871989	34.675687
1090.269087	77222.868627	34.680704
1091.778901	77333.856473	34.685722
1092.575107	77436.919156	34.690740
1093.832083	77553.371132	34.695757
1094.640985	77663.751757	34.700775
1096.300423	77759.789710	34.705792
1096.971462	77874.813533	34.710810
1098.347722	77961.796226	34.715828
1099.153271	78056.941176	34.720845
1100.235927	78143.244500	34.725863
1101.379138	78243.342373	34.730880
1101.467222	78356.078825	34.735898
1102.606751	78459.306974	34.740916
1104.369943	78566.784979	34.745933
1105.038557	78675.063374	34.750951
1106.826720	78772.533043	34.755968
1107.250550	78890.673714	34.760986
1108.377221	78991.245612	34.766004
1109.185831	79104.073848	34.771021
1110.388756	79223.065914	34.776039
1111.433231	79343.916893	34.781056
1112.185382	79458.999935	34.786074
1113.388823	79577.873881	34.791092
1114.107406	79704.334832	34.796109
1115.126775	79844.142755	34.801127
1116.685289	79957.109251	34.806144
1117.629679	80086.494846	34.811162
1119.106580	80220.088549	34.816180
1120.195828	80356.545008	34.821197
1121.520456	80475.859987	34.826215
1122.819060	80598.827101	34.831232
1123.571035	80727.868051	34.836250
1125.269841	80845.090234	34.841268
1126.481709	80962.504305	34.846285
1127.608092	81098.352918	34.851303
1128.854551	81209.688117	34.856320
1130.335872	81321.359525	34.861338
1131.660395	81441.002484	34.866356
1132.642981	81557.141538	34.871373
1133.876670	81663.828625	34.876391
1135.495939	81777.079886	34.881408
1136.045042	81891.393293	34.886426
1137.146050	82005.328765	34.891444
1138.342207	82121.418045	34.896461
1139.129610	82234.589157	34.901479
1140.520175	82339.503667	34.906496
1141.591629	82473.587296	34.911514
1143.022080	82592.809128	34.916532
1144.014380	82704.249651	34.921549
1145.094851	82816.075022	34.926567
1146.640501	82933.674739	34.931584
1147.561124	83054.984319	34.936602
1148.651962	83154.855146	34.941620
1150.124803	83277.886274	34.946637
1151.060633	83395.952242	34.951655
1152.592838	83502.550695	34.956672
1153.303341	83632.981802	34.961690
1154.407748	83736.450505	34.966708
1155.656869	83845.403287	34.971725
1156.159899	83970.400832	34.976743
1157.786245	84085.724527	34.981760
1158.694959	84215.331128	34.986778
1159.846512	84320.913166	34.991796
1161.182725	84430.740252	34.996813
1161.999270	84530.243969	35.001831
1163.122388	84644.379960	35.006848
1163.980315	84757.148841	35.011866
1165.217994	84868.150876	35.016884
1166.173027	84989.409245	35.021901
1167.384972	85113.504200	35.026919
1168.606724	85229.549714	35.031936
1169.687560	85352.889249	35.036954
1171.116021	85474.391244	35.041972
1171.983643	85589.230518	35.046989
1173.207983	85721.186131	35.052007
1174.562909	85850.428314	35.057024
1175.746584	85981.051589	35.062042
1176.961769	86092.974104	35.067060
1178.310986	86219.197137	35.072077
1179.081057	86343.597177	35.077095
1180.508019	86467.539406	35.082112
1181.478377	86600.963524	35.087130
1182.735464	86727.292741	35.092148
1184.238759	86861.620134	35.097165
1184.854531	86990.759146	35.102183
1186.278767	87116.463396	35.107200
1187.453314	87241.948839	35.112218
1188.913973	87372.416458	35.117236
1190.026315	87510.053887	35.122253
1191.334496	87649.886851	35.127271
1192.403425	87758.230770	35.132288
1193.816823	87898.636693	35.137306
1194.926758	88031.345645	35.142324
1196.572642	88157.988242	35.147341
1197.471930	88299.243664	35.152359
1198.905997	88425.099467	35.157376
1200.058441	88548.439753	35.162394
1200.814215	88681.133143	35.167412
1202.149782	88805.590350	35.172429
1203.189463	88949.129501	35.177447
1204.735178	89079.480135	35.182464
1205.578444	89214.920021	35.187482
1206.724614	89358.982477	35.192500
1208.055999	89495.434194	35.197517
1209.263453	89636.238314	35.202535
1210.782040	89766.426658	35.207552
1211.772018	89899.532952	35.212570
1213.220646	90031.378232	35.217588
1214.557451	90167.757431	35.222605
1215.508363	90303.275532	35.227623
1217.349775	90433.049752	35.232640
1218.185735	90569.814661	35.237658
1219.343656	90695.639035	35.242676
1220.914365	90816.845084	35.247693
1221.895582	90948.529919	35.252711
1223.202992	91070.291503	35.257728
1224.899330	91210.635978	35.262746
1226.041264	91316.304592	35.267764
1226.993996	91428.201680	35.272781
1228.025305	91547.075312	35.277799
1229.386156	91655.917233	35.282816
1230.523727	91777.526350	35.287834
1231.472728	91887.098970	35.292852
1233.094937	92007.114427	35.297869
1234.123566	92131.980993	35.302887
1235.382336	92241.765441	35.307904
1236.561679	92361.948119	35.312922
1237.706840	92488.221224	35.317940
1239.038268	92608.444316	35.322957
1239.871382	92736.166215	35.327975
1241.250263	92864.225843	35.332992
1242.406817	92989.367873	35.338010
1243.470879	93126.776561	35.343028
1244.951620	93259.964401	35.348045
1246.150051	93398.940967	35.353063
1247.312540	93523.193260	35.358080
1248.694381	93665.431325	35.363098
1249.896691	93795.497824	35.368116
1251.234958	93934.600996	35.373133
1252.212549	94075.248785	35.378151
1253.808890	94208.923638	35.383168
1255.463898	94345.803172	35.388186
1256.403176	94486.472304	35.393204
1257.621193	94613.865520	35.398221
1259.081032	94747.470432	35.403239
1260.630620	94889.708641	35.408256
1261.746373	95020.106006	35.413274
1263.137317	95154.363174	35.418292
1264.455155	95272.736869	35.423309
1265.333903	95419.335814	35.428327
1266.587806	95565.407986	35.433344
1268.354983	95682.757259	35.438362
1269.288368	95818.299339	35.443380
1270.437480	95953.890175	35.448397
1272.060284	96083.669119	35.453415
1273.297023	96218.159601	35.458432
1274.670855	96351.971214	35.463450
1275.777258	96491.171445	35.468468
1277.022427	96630.249262	35.473485
1278.052894	96772.063223	35.478503
1279.737107	96888.672882	35.483520
1281.382609	97014.531519	35.488538
1282.263008	97179.834880	35.493556
1283.703934	97301.754910	35.498573
1285.042215	97435.844300	35.503591
1286.357405	97570.330373	35.508608
1287.781012	97710.531501	35.513626
1288.905674	97842.645541	35.518644
1290.312471	97964.479674	35.523661
1291.116052	98104.743844	35.528679
1292.482042	98237.764432	35.533696
1293.939889	98375.022494	35.538714
1295.177349	98492.072034	35.543732
1296.453780	98626.735010	35.548749
1297.634055	98727.864973	35.553767
1299.281556	98859.092022	35.558784
1300.208399	98978.958107	35.563802
1301.441754	99097.377933	35.568820
1302.776033	99211.866185	35.573837
1303.790543	99349.143644	35.578855
1305.260150	99471.260549	35.583872
1306.426106	99601.632068	35.588890
1307.740994	99733.220689	35.593908
1308.711571	99862.334099	35.598925
1310.109684	100000.142866	35.603943
1311.530343	100139.049744	35.608960
1312.856980	100268.374563	35.613978
1314.215259	100409.121450	35.618996
1315.566038	100540.854510	35.624013
1316.776149	100686.074474	35.629031
1318.067915	100834.939386	35.634048
1319.532897	100968.649746	35.639066
1320.532084	101129.363010	35.644084
1322.165603	101269.875257	35.649101
1323.537978	101416.624167	35.654119
1324.738192	101556.561658	35.659136
1326.002038	101708.910269	35.664154
1327.362039	101844.799970	35.669172
1328.826807	101987.659180	35.674189
1329.925395	102148.116936	35.679207
1331.335557	102292.771019	35.684224
1333.001722	102426.698253	35.689242
1334.155749	102581.733891	35.694260
1335.772891	102733.735665	35.699277
1336.865647	102885.815451	35.704295
1338.401146	103028.024387	35.709312
1339.879553	103172.679407	35.714330
1341.052402	103328.976212	35.719348
1342.565533	103468.059172	35.724365
1343.853633	103619.188825	35.729383
1345.385584	103762.579751	35.734400
1346.812297	103899.122570	35.739418
1348.308858	104055.999221	35.744436
1349.918780	104195.109074	35.749453
1351.111460	104330.166564	35.754471
1352.291435	104463.467666	35.759488
1353.840649	104596.938644	35.764506
1355.069320	104748.015383	35.769524
1356.765688	104886.754878	35.774541
1357.941221	105038.000120	35.779559
1359.135497	105177.561517	35.784576
1360.359737	105309.461826	35.789594
1361.758842	105459.655382	35.794612
1363.209686	105611.873050	35.799629
1364.583628	105748.295726	35.804647
1365.813233	105890.703455	35.809664
1367.262078	106031.798851	35.814682
1368.720025	106175.209850	35.819700
1369.974678	106295.808194	35.824717
1371.159442	106424.607353	35.829735
1372.087384	106564.681204	35.834752
1373.633605	106695.645700	35.839770
1374.935495	106827.004150	35.844788
1376.365108	106957.203864	35.849805
1377.396236	107104.890511	35.854823
1378.758004	107251.962261	35.859840
1380.192099	107397.086814	35.864858
1381.360325	107552.950192	35.869876
1383.097784	107686.883246	35.874893
1384.216920	107841.712037	35.879911
1385.502746	107987.066242	35.884928
1387.181991	108135.687835	35.889946
1388.115239	108296.985653	35.894964
1389.661727	108452.592207	35.899981
1391.078343	108598.416647	35.904999
1392.346674	108762.968104	35.910016
1393.988538	108917.651101	35.915034
1394.812372	109089.553965	35.920052
1396.544560	109247.845026	35.925069
1397.878359	109397.415368	35.930087
1399.305430	109572.700567	35.935104
1400.838507	109735.235459	35.940122
1401.875171	109896.508488	35.945140
1403.513528	110052.370211	35.950157
1404.736209	110226.287451	35.955175
1406.334243	110397.525843	35.960192
1408.248365	110553.214019	35.965210
1409.474005	110735.711014	35.970228
1411.102692	110890.294701	35.975245
1412.421566	111059.012233	35.980263
1413.919435	111215.137890	35.985280
1415.605829	111375.792042	35.990298
1416.921902	111545.735012	35.995316
1418.744513	111705.458172	36.000333
1420.204894	111862.821897	36.005351
1421.701097	112016.667799	36.010368
1423.465606	112158.736187	36.015386
1424.267236	112331.197042	36.020404
1425.999575	112476.899491	36.025421
1427.346304	112641.401255	36.030439
1428.543114	112799.205292	36.035456
1430.317714	112956.450080	36.040474
1431.938399	113118.012233	36.045492
1433.176825	113262.329167	36.050509
1434.479902	113434.312859	36.055527
1436.030190	113592.483562	36.060544
1437.801773	113740.852279	36.065562
1439.130619	113899.237368	36.070580
1440.622793	114045.310029	36.075597
1442.068141	114207.286934	36.080615
1443.309951	114368.911066	36.085632
1444.960762	114504.889271	36.090650
1446.222293	114649.672682	36.095668
1447.410698	114790.176350	36.100685
1448.405956	114930.034110	36.105703
1449.798118	115063.207620	36.110720
1451.558038	115222.121326	36.115738
1452.514482	115379.378415	36.120756
1453.616234	115528.123710	36.125773
1455.172598	115673.746152	36.130791
1456.601233	115840.269153	36.135808
1458.143934	115994.891881	36.140826
1459.546472	116169.448873	36.145844
1461.343766	116331.358192	36.150861
1462.601887	116492.708446	36.155879
1463.777308	116661.176404	36.160896
1465.494487	116823.886656	36.165914
1466.876838	116992.026360	36.170932
1468.356769	117154.687786	36.175949
1470.375791	117329.287743	36.180967
1471.702394	117484.808598	36.185984
1473.171429	117646.119979	36.191002
1474.645709	117822.411702	36.196020
1476.011543	117984.172148	36.201037
1477.299722	118145.395112	36.206055
1478.665719	118329.235689	36.211072
1480.673341	118491.036651	36.216090
1481.908319	118670.430379	36.221108
1483.317620	118836.399822	36.226125
1485.155665	118997.135529	36.231143
1486.826204	119182.067183	36.236160
1488.567770	119346.695437	36.241178
1489.939855	119515.315519	36.246196
1491.976818	119680.601799	36.251213
1493.493033	119846.940658	36.256231
1494.421068	120018.667558	36.261248
1496.094189	120177.594200	36.266266
1497.456961	120348.076450	36.271284
1498.823864	120520.370137	36.276301
1500.418179	120683.029323	36.281319
1501.993890	120858.432803	36.286336
1503.381690	121025.762085	36.291354
1505.030788	121197.749454	36.296372
1506.377368	121369.393414	36.301389
1508.303982	121545.657601	36.306407
1509.502490	121719.455042	36.311424
1511.094266	121880.602303	36.316442
1512.446211	122054.744862	36.321460
1513.990117	122233.379481	36.326477
1515.580573	122416.428032	36.331495
1516.886536	122581.069890	36.336512
1518.441214	122753.994330	36.341530
1519.862026	122925.459324	36.346548
1521.460604	123109.321963	36.351565
1522.982911	123287.422522	36.356583
1524.503266	123467.272437	36.361600
1525.971744	123640.925629	36.366618
1527.400635	123810.811848	36.371636
1528.955068	123950.876508	36.376653
1530.664165	124106.787698	36.381671
1531.939129	124272.825551	36.386688
1533.435751	124431.837560	36.391706
1534.678583	124600.783079	36.396724
1536.405030	124763.345062	36.401741
1537.971717	124938.270375	36.406759
1538.780848	125101.828780	36.411776
1540.663667	125269.676197	36.416794
1542.150563	125436.156242	36.421812
1543.597641	125633.271502	36.426829
1545.414796	125789.871976	36.431847
1546.787395	125973.562200	36.436864
1548.158925	126157.038504	36.441882
1549.620443	126339.197060	36.446900
1551.296945	126538.119177	36.451917
1553.143722	126692.123427	36.456935
1554.631675	126921.023365	36.461952
1556.475906	127075.245535	36.466970
1558.027617	127256.534539	36.471988
1559.585323	127447.349726	36.477005
1561.389075	127627.093727	36.482023
1563.048875	127812.549543	36.487040
1564.531926	127993.943021	36.492058
1566.073872	128170.983291	36.497076
1567.910070	128352.500392	36.502093
1569.569389	128526.433347	36.507111
1570.835984	128713.211841	36.512128
1573.014066	128897.743901	36.517146
1574.453884	129071.119763	36.522164
1575.683773	129264.659977	36.527181
1577.538940	129436.236596	36.532199
1578.881159	129620.678232	36.537216
1580.999820	129791.391748	36.542234
1582.483242	129979.373200	36.547252
1583.910876	130153.416541	36.552269
1585.591095	130331.322834	36.557287
1587.146969	130525.453496	36.562304
1588.793648	130699.110724	36.567322
1590.572917	130878.195655	36.572340
1592.146571	131065.308604	36.577357
1593.968210	131240.981136	36.582375
1595.564724	131413.966636	36.587392
1597.390226	131595.633344	36.592410
1598.770583	131772.190136	36.597428
1599.914051	131960.758354	36.602445
1601.880581	132118.422652	36.607463
1603.204641	132297.956364	36.612480
1605.188264	132479.983753	36.617498
1606.872475	132673.969517	36.622516
1608.295344	132837.083524	36.627533
1609.919262	133006.007398	36.632551
1611.727299	133177.905838	36.637568
1613.503349	133346.262762	36.642586
1614.774122	133513.788682	36.647604
1616.203800	133676.019510	36.652621
1618.018621	133815.472150	36.657639
1619.589130	133976.288580	36.662656
1620.823030	134131.622376	36.667674
1622.506676	134310.680893	36.672692
1623.924698	134465.923907	36.677709
1625.491732	134640.796358	36.682727
1626.772682	134817.261149	36.687744
1628.490149	134989.197548	36.692762
1630.189810	135165.838720	36.697780
1631.329044	135354.468075	36.702797
1633.355186	135531.008947	36.707815
1634.791135	135720.011709	36.712832
1636.235145	135897.445561	36.717850
1637.992842	136077.415632	36.722868
1639.419473	136269.464578	36.727885
1641.784834	136449.707920	36.732903
1643.024066	136634.490257	36.737920
1644.780695	136822.422866	36.742938
1646.444168	137025.729640	36.747956
1648.297198	137218.895597	36.752973
1650.066479	137395.209814	36.757991
1651.305041	137587.956248	36.763008
1652.941679	137781.857245	36.768026
1654.693494	137977.299906	36.773044
1656.425800	138176.928805	36.778061
1658.130647	138367.996922	36.783079
1659.879085	138557.513321	36.788096
1661.719945	138758.269432	36.793114
1663.415572	138947.923446	36.798132
1664.978227	139152.515514	36.803149
1666.798150	139334.903501	36.808167
1668.467433	139539.785449	36.813184
1669.939741	139727.642349	36.818202
1672.367879	139927.083828	36.823220
1673.645684	140119.612403	36.828237
1675.693348	140314.187066	36.833255
1677.626481	140504.434264	36.838272
1679.264630	140692.245545	36.843290
1680.891705	140870.212534	36.848308
1682.326990	141071.618935	36.853325
1683.759234	141252.863538	36.858343
1685.602512	141447.401963	36.863360
1687.041550	141635.770371	36.868378
1688.949386	141833.000530	36.873396
1690.343185	142039.755645	36.878413
1692.389944	142224.964132	36.883431
1693.745775	142416.151549	36.888448
1695.785975	142615.723150	36.893466
1697.660858	142816.589733	36.898484
1698.948713	143014.762515	36.903501
1700.553795	143205.991351	36.908519
1702.210922	143404.576971	36.913536
1703.810048	143596.214773	36.918554
1705.467880	143777.679417	36.923572
1707.067699	143977.634029	36.928589
1708.551390	144160.738271	36.933607
1710.391661	144343.660231	36.938624
1712.061019	144528.258153	36.943642
1713.821858	144717.519723	36.948660
1715.139410	144913.748076	36.953677
1717.054891	145100.059488	36.958695
1718.917713	145291.171614	36.963712
1720.531529	145481.969547	36.968730
1722.468098	145669.941493	36.973748
1724.217645	145875.296967	36.978765
1726.039280	146067.586541	36.983783
1727.487360	146257.249384	36.988800
1729.043202	146447.377939	36.993818
1730.833969	146651.198202	36.998836
1732.552034	146867.846623	37.003853
1734.160585	147068.757727	37.008871
1735.969085	147280.552418	37.013888
1737.817655	147482.530861	37.018906
1739.826341	147690.645798	37.023924
1741.305000	147896.868763	37.028941
1743.377553	148098.232461	37.033959
1745.051918	148308.179224	37.038976
1746.765001	148514.077414	37.043994
1748.792781	148711.471678	37.049012
1749.935192	148937.961273	37.054029
1751.968632	149132.441602	37.059047
1754.126847	149346.945389	37.064064
1755.570038	149554.452381	37.069082
1757.753914	149770.488831	37.074100
1759.164908	149980.944753	37.079117
1760.895102	150188.511678	37.084135
1762.876845	150408.869385	37.089152
1764.390380	150614.166180	37.094170
1766.714687	150816.787386	37.099188
1768.197176	151047.484737	37.104205
1770.173960	151251.964041	37.109223
1772.098411	151448.935080	37.114240
1773.828051	151661.962910	37.119258
1776.122930	151874.699541	37.124276
1777.311448	152075.163499	37.129293
1779.387043	152281.522566	37.134311
1781.233028	152497.098306	37.139328
1782.785699	152707.346489	37.144346
1785.021518	152914.279961	37.149364
1786.165496	153129.628976	37.154381
1788.286828	153333.920806	37.159399
1790.511286	153539.604834	37.164416
1792.185568	153741.979633	37.169434
1793.909481	153938.680439	37.174452
1795.677477	154148.662686	37.179469
1797.483674	154354.164580	37.184487
1799.289984	154564.498365	37.189504
1801.045047	154759.449378	37.194522
1802.917214	154940.195129	37.199540
1804.354400	155126.665774	37.204557
1806.406853	155308.589398	37.209575
1808.518215	155493.141929	37.214592
1810.020345	155661.359848	37.219610
1811.865317	155843.179824	37.224628
1813.476344	156046.275933	37.229645
1815.352389	156225.772698	37.234663
1817.360117	156422.366905	37.239680
1818.990542	156603.629080	37.244698
1820.446290	156795.152462	37.249716
1821.975667	157000.498857	37.254733
1823.820451	157197.148760	37.259751
1825.926316	157392.338198	37.264768
1827.450912	157608.758568	37.269786
1829.191063	157807.672943	37.274804
1831.056471	158022.266603	37.279821
1833.086582	158223.191534	37.284839
1834.910088	158434.954044	37.289856
1836.449886	158648.373294	37.294874
1838.866472	158851.624438	37.299892
1840.238980	159072.807930	37.304909
1842.570766	159287.348079	37.309927
1844.458591	159494.972967	37.314944
1846.157687	159708.043733	37.319962
1848.062159	159922.186429	37.324980
1849.858534	160142.497837	37.329997
1851.635445	160361.304679	37.335015
1853.806876	160579.530333	37.340032
1855.512134	160794.635686	37.345050
1857.566631	161001.431434	37.350068
1859.556390	161217.597469	37.355085
1861.416422	161439.175002	37.360103
1863.811444	161644.791811	37.365120
1865.513033	161859.460359	37.370138
1867.405211	162072.819104	37.375156
1868.945377	162284.446882	37.380173
1870.949925	162487.797104	37.385191
1872.980904	162707.021936	37.390208
1874.807262	162930.884118	37.395226
1876.746399	163126.081189	37.400244
1878.926586	163335.432272	37.405261
1880.807234	163558.503448	37.410279
1882.556671	163764.983136	37.415296
1884.583403	163971.686314	37.420314
1886.339217	164188.452726	37.425332
1888.415547	164397.712291	37.430349
1890.420239	164607.529775	37.435367
1892.335370	164811.528699	37.440384
1893.688060	165032.004001	37.445402
1896.016209	165227.493049	37.450420
1897.865387	165432.203445	37.455437
1899.721266	165651.638708	37.460455
1901.524426	165855.369496	37.465472
1903.520126	166077.270952	37.470490
1905.203923	166261.985744	37.475508
1906.880997	166454.439233	37.480525
1908.577608	166647.131598	37.485543
1910.524315	166837.870096	37.490560
1912.297050	167045.708942	37.495578
1914.406024	167229.764943	37.500596
1915.952360	167431.084549	37.505613
1917.747050	167634.344451	37.510631
1919.538625	167844.848283	37.515648
1920.906712	168049.915790	37.520666
1923.025992	168270.123733	37.525684
1925.126766	168494.204460	37.530701
1926.977773	168717.298759	37.535719
1929.165700	168921.226164	37.540736
1931.003539	169145.111472	37.545754
1932.940543	169365.988907	37.550772
1934.998887	169585.047210	37.555789
1936.488113	169806.213884	37.560807
1938.956024	170025.932713	37.565824
1940.560405	170243.506652	37.570842
1942.961269	170470.519510	37.575860
1945.117832	170694.439392	37.580877
1947.238191	170919.228871	37.585895
1949.356404	171138.629002	37.590912
1951.015915	171367.299622	37.595930
1952.943566	171572.385976	37.600948
1955.339944	171795.373531	37.605965
1957.145480	172035.872600	37.610983
1959.334080	172245.792113	37.616000
1961.334296	172470.964789	37.621018
1963.490304	172683.784025	37.626036
1965.044934	172910.755113	37.631053
1966.823592	173135.662300	37.636071
1969.305095	173349.359500	37.641088
1971.331110	173578.555671	37.646106
1973.222279	173804.603175	37.651124
1975.518155	174021.403351	37.656141
1977.051710	174246.990000	37.661159
1979.268704	174466.608647	37.666176
1981.656056	174697.821684	37.671194
1983.885739	174901.443868	37.676212
1985.779505	175135.655503	37.681229
1987.732673	175352.606056	37.686247
1989.944456	175559.279050	37.691264
1991.764804	175793.024068	37.696282
1994.226882	175980.351139	37.701300
1996.174797	176200.491304	37.706317
1997.906802	176411.012591	37.711335
2000.131616	176631.149199	37.716352
2001.696700	176840.506656	37.721370
2003.926388	177046.524650	37.726388
2006.101993	177253.757487	37.731405
2008.260473	177467.730717	37.736423
2010.446317	177665.778836	37.741440
2011.954308	177878.563357	37.746458
2013.968487	178067.087461	37.751476
2016.083218	178256.814411	37.756493
2017.545062	178428.376558	37.761511
2019.703385	178632.942078	37.766528
2021.487397	178824.830137	37.771546
2023.689209	179002.138672	37.776564
2025.158387	179198.150970	37.781581
2027.174681	179396.843198	37.786599
2029.394295	179601.403715	37.791616
2031.248052	179811.516916	37.796634
2033.149329	180010.585529	37.801652
2035.190037	180220.341220	37.806669
2036.721526	180432.792383	37.811687
2039.099912	180648.789653	37.816704
2041.314214	180855.501268	37.821722
2043.442345	181088.402437	37.826740
2045.724364	181303.898105	37.831757
2047.311257	181521.497142	37.836775
2049.764410	181733.922714	37.841792
2051.462545	181963.331517	37.846810
2053.684504	182179.906884	37.851828
2055.627275	182396.197735	37.856845
2057.702768	182622.809508	37.861863
2060.098384	182851.845888	37.866880
2062.371889	183071.995613	37.871898
2064.424562	183289.834122	37.876916
2066.856073	183512.549429	37.881933
2068.843189	183734.701938	37.886951
2071.173442	183941.232203	37.891968
2073.258686	184156.570172	37.896986
2075.368781	184370.991656	37.902004
2077.568757	184588.559425	37.907021
2079.602945	184799.340643	37.912039
2081.629159	185019.767695	37.917056
2083.957180	185230.656600	37.922074
2085.978184	185438.562523	37.927092
2088.024627	185660.829425	37.932109
2090.245008	185872.690099	37.937127
2092.762724	186078.718317	37.942144
2094.884448	186297.156954	37.947162
2096.997479	186507.058101	37.952180
2099.267849	186714.930332	37.957197
2101.271369	186927.312528	37.962215
2103.335144	187128.049877	37.967232
2105.391707	187341.631084	37.972250
2107.646951	187542.174906	37.977268
2109.923089	187758.388037	37.982285
2111.967207	187968.598672	37.987303
2114.255893	188163.429511	37.992320
2116.465399	188375.671505	37.997338
2118.742191	188569.985655	38.002356
2120.805709	188769.055109	38.007373
2122.560335	188970.331712	38.012391
2124.914714	189172.275447	38.017408
2127.146670	189369.442609	38.022426
2129.217824	189539.732958	38.027444
2131.098588	189713.036323	38.032461
2132.896075	189890.021018	38.037479
2134.926641	190069.697818	38.042496
2137.017120	190256.929244	38.047514
2138.729366	190457.444806	38.052532
2140.791407	190641.205086	38.057549
2142.484395	190838.628833	38.062567
2144.500922	191039.809243	38.067584
2146.415396	191247.605803	38.072602
2148.577732	191445.071815	38.077620
2150.954270	191671.401432	38.082637
2152.502258	191885.921505	38.087655
2154.681266	192092.499501	38.092672
2156.879603	192323.352985	38.097690
2159.029810	192546.308734	38.102708
2161.819121	192772.793761	38.107725
2163.655291	192985.775426	38.112743
2166.097465	193213.256688	38.117760
2167.847854	193446.179022	38.122778
2170.128346	193677.343131	38.127796
2172.676559	193895.546112	38.132813
2174.890657	194118.549614	38.137831
2177.226929	194349.390722	38.142848
2179.554667	194574.561164	38.147866
2181.554212	194813.567673	38.152884
2183.873885	195028.055163	38.157901
2186.006008	195265.418270	38.162919
2188.439463	195479.381969	38.167936
2190.691265	195710.395026	38.172954
2192.815281	195935.946538	38.177972
2195.086979	196171.159524	38.182989
2196.957394	196397.717881	38.188007
2199.437415	196631.681520	38.193024
2201.786448	196861.922848	38.198042
2204.049543	197092.991128	38.203060
2206.329357	197316.835956	38.208077
2208.736299	197549.152676	38.213095
2211.049520	197767.320732	38.218112
2213.191143	198007.170011	38.223130
2215.578279	198230.481364	38.228148
2218.139893	198444.068984	38.233165
2219.947349	198668.819531	38.238183
2222.540863	198902.051914	38.243200
2225.036803	199119.498527	38.248218
2226.896174	199339.192039	38.253236
2229.373245	199552.987940	38.258253
2231.532985	199778.931207	38.263271
2233.607198	199993.211618	38.268288
2235.707325	200210.611217	38.273306
2238.160578	200446.436555	38.278324
2240.560102	200660.401486	38.283341
2242.603262	200884.603563	38.288359
2245.130263	201099.159275	38.293376
2247.202146	201314.194185	38.298394
2248.987663	201524.261558	38.303412
2251.463754	201721.514335	38.308429
2253.299195	201915.175679	38.313447
2255.368714	202110.336474	38.318464
2257.492088	202321.698806	38.323482
2259.738981	202524.030057	38.328500
2262.401466	202725.585314	38.333517
2264.283814	202931.225373	38.338535
2266.669600	203139.350450	38.343552
2268.830866	203345.265143	38.348570
2270.720246	203564.678937	38.353588
2273.071805	203788.107660	38.358605
2275.248555	204020.539444	38.363623
2277.224075	204237.860423	38.368640
2279.426092	204478.198293	38.373658
2281.555927	204713.382213	38.378676
2283.808460	204943.305054	38.383693
2285.892033	205195.140023	38.388711
2287.961782	205434.969728	38.393728
2290.539619	205678.477313	38.398746
2292.371971	205948.050949	38.403764
2294.777702	206194.634580	38.408781
2297.148751	206468.301593	38.413799
2299.720185	206719.926171	38.418816
2301.905092	206963.742605	38.423834
2304.415903	207235.118729	38.428852
2306.937147	207482.666909	38.433869
2309.165018	207746.905159	38.438887
2311.545191	208016.502933	38.443904
2314.246648	208271.502918	38.448922
2316.628905	208513.796426	38.453940
2318.817097	208768.029344	38.458957
2321.002553	209035.809108	38.463975
2323.241449	209287.459112	38.468992
2325.988161	209559.608079	38.474010
2328.273632	209819.936202	38.479028
2330.821725	210066.767071	38.484045
2333.081768	210340.837422	38.489063
2335.224654	210599.363336	38.494080
2338.030004	210854.078301	38.499098
2340.174599	211118.864811	38.504116
2342.582767	211371.232752	38.509133
2344.933416	211631.697743	38.514151
2347.396005	211900.182233	38.519168
2349.664867	212155.736531	38.524186
2351.927452	212420.865239	38.529204
2354.891506	212674.927586	38.534221
2356.938720	212936.918681	38.539239
2359.484857	213195.061134	38.544256
2362.244815	213443.344256	38.549274
2364.374444	213711.495507	38.554292
2366.530410	213959.114595	38.559309
2368.724195	214209.305871	38.564327
2371.298104	214479.941682	38.569344
2373.805208	214716.030862	38.574362
2375.771233	214953.819044	38.579380
2378.046650	215193.361858	38.584397
2380.364911	215417.904686	38.589415
2382.363457	215670.138366	38.594432
2384.532011	215891.672131	38.599450
2386.947792	216143.130443	38.604468
2389.306958	216392.567258	38.609485
2391.382921	216628.680685	38.614503
2393.581603	216889.558707	38.619520
2395.988368	217153.693090	38.624538
2397.973544	217414.099076	38.629556
2400.296872	217686.983852	38.634573
2402.830411	217953.069121	38.639591
2404.608109	218233.812787	38.644608
2407.300854	218503.137913	38.649626
2409.360301	218794.021826	38.654644
2411.980972	219092.296333	38.659661
2414.273278	219377.051272	38.664679
2417.129279	219662.378216	38.669696
2419.474079	219944.409945	38.674714
2421.658097	220249.449689	38.679732
2424.591473	220539.351393	38.684749
2426.984838	220820.324943	38.689767
2429.574263	221131.589107	38.694784
2432.242018	221406.541057	38.699802
2434.446997	221715.697381	38.704820
2437.227925	222008.854053	38.709837
2439.698157	222355.148445	38.714855
2442.019026	222654.754567	38.719872
2444.523849	222941.927358	38.724890
2446.696553	223247.323886	38.729908
2449.586819	223536.710635	38.734925
2452.280072	223830.408753	38.739943
2454.238078	224125.862492	38.744960
2457.452970	224413.740809	38.749978
2459.826389	224722.768184	38.754996
2462.591707	225021.093953	38.760013
2465.164532	225305.623477	38.765031
2467.713307	225594.868702	38.770048
2470.425456	225877.359203	38.775066
2472.670010	226172.483012	38.780084
2475.101219	226456.124754	38.785101
2477.863280	226749.289315	38.790119
2480.134158	227043.396224	38.795136
2482.982008	227324.613067	38.800154
2485.404466	227624.310539	38.805172
2487.862706	227899.800707	38.810189
2490.519389	228190.269592	38.815207
2492.949403	228485.600719	38.820224
2495.533960	228773.873515	38.825242
2497.662347	229051.095827	38.830260
2500.175605	229338.391325	38.835277
2502.676058	229636.432650	38.840295
2504.978080	229923.331788	38.845312
2507.524757	230200.135873	38.850330
2510.067221	230480.903426	38.855348
2512.791499	230737.033214	38.860365
2514.834922	230990.604919	38.865383
2517.111302	231253.689790	38.870400
2520.102251	231513.970061	38.875418
2521.912567	231793.410042	38.880436
2524.098280	232055.571869	38.885453
2526.597265	232335.971043	38.890471
2528.687547	232626.188521	38.895488
2531.129748	232909.163565	38.900506
2533.702501	233205.274828	38.905524
2536.056390	233495.554778	38.910541
2538.666919	233801.338488	38.915559
2541.176154	234109.069464	38.920576
2543.916084	234399.265546	38.925594
2546.400242	234716.450501	38.930612
2548.761179	235023.242701	38.935629
2551.487172	235330.435165	38.940647
2553.833535	235645.105065	38.945664
2556.588226	235967.635574	38.950682
2559.015531	236283.361355	38.955700
2561.941817	236593.802309	38.960717
2564.571293	236917.244581	38.965735
2566.828123	237241.889845	38.970752
2569.521374	237544.369910	38.975770
2572.236082	237873.084572	38.980788
2574.713827	238198.967692	38.985805
2577.644539	238521.351138	38.990823
2580.198781	238841.331463	38.995840
2583.428191	239168.800121	39.000858
2585.957824	239493.789887	39.005876
2588.480273	239820.381894	39.010893
2591.106490	240130.880521	39.015911
2593.513661	240456.908431	39.020928
2596.546670	240772.881447	39.025946
2599.137968	241100.964764	39.030964
2601.472106	241426.778362	39.035981
2604.103122	241744.773465	39.040999
2606.945893	242077.213811	39.046016
2609.697507	242400.550922	39.051034
2612.051498	242720.929281	39.056052
2614.929483	243043.359064	39.061069
2617.891103	243365.268428	39.066087
2620.218162	243694.848421	39.071104
2623.237571	244001.179906	39.076122
2625.861905	244330.612842	39.081140
2628.063430	244658.335570	39.086157
2630.718591	244969.934140	39.091175
2633.558536	245300.071971	39.096192
2636.034723	245620.793817	39.101210
2638.818627	245953.609195	39.106228
2641.192412	246272.926365	39.111245
2644.012267	246593.900859	39.116263
2646.065706	246939.814137	39.121280
2649.033837	247243.595651	39.126298
2651.623346	247557.928389	39.131316
2653.714759	247860.859460	39.136333
2656.435623	248158.027005	39.141351
2659.013462	248467.791360	39.146368
2661.331057	248764.795395	39.151386
2663.487688	249092.179970	39.156404
2666.153297	249399.697025	39.161421
2669.000834	249735.152732	39.166439
2671.427184	250067.500706	39.171456
2674.153453	250378.286853	39.176474
2676.877572	250719.276304	39.181492
2679.521145	251046.867218	39.186509
2682.038881	251390.329305	39.191527
2684.380583	251733.896187	39.196544
2687.399474	252078.296357	39.201562
2690.072299	252421.862974	39.206580
2692.569452	252766.855192	39.211597
2695.583700	253122.333338	39.216615
2698.048491	253477.797612	39.221632
2701.092374	253821.054125	39.226650
2704.150499	254180.947317	39.231668
2706.551109	254535.839534	39.236685
2709.551678	254887.563725	39.241703
2711.957797	255253.633298	39.246720
2715.013670	255614.215368	39.251738
2717.838337	255966.629787	39.256756
2720.717426	256319.772856	39.261773
2723.755408	256680.918479	39.266791
2726.217750	257039.691861	39.271808
2728.828957	257396.029028	39.276826
2731.547673	257766.371877	39.281844
2734.077707	258123.408921	39.286861
2737.115241	258496.344311	39.291879
2739.759032	258859.892907	39.296896
2742.816382	259223.630576	39.301914
2745.378368	259602.587198	39.306932
2748.275061	259971.254107	39.311949
2751.223457	260334.172348	39.316967
2753.973663	260715.031396	39.321984
2756.656046	261076.265388	39.327002
2759.409485	261443.661475	39.332020
2762.056919	261813.030841	39.337037
2765.164658	262187.484553	39.342055
2767.735505	262569.339793	39.347072
2770.678687	262934.599238	39.352090
2773.106796	263313.531251	39.357108
2776.205557	263692.001849	39.362125
2779.438624	264055.844876	39.367143
2781.622871	264442.640898	39.372160
2784.473551	264804.792444	39.377178
2787.771538	265187.475401	39.382196
2790.333438	265557.345129	39.387213
2793.161335	265924.937599	39.392231
2795.692600	266302.637017	39.397248
2798.842781	266650.923498	39.402266
2801.376427	266996.437325	39.407284
2804.006532	267338.405088	39.412301
2806.547524	267666.694867	39.417319
2809.189353	268012.319304	39.422336
2812.151427	268367.927542	39.427354
2814.349360	268716.747324	39.432372
2817.062820	269062.869142	39.437389
2819.868540	269431.839517	39.442407
2822.458037	269789.031801	39.447424
2825.255685	270166.666392	39.452442
2827.951619	270530.320046	39.457460
2830.823048	270917.647405	39.462477
2833.729749	271291.022912	39.467495
2836.118217	271674.997627	39.472512
2838.995697	272073.451194	39.477530
2842.020798	272446.554351	39.482548
2844.602223	272858.569666	39.487565
2847.717376	273241.134256	39.492583
2850.245949	273652.116616	39.497600
2853.455202	274043.024202	39.502618
2856.193519	274457.199738	39.507636
2858.641439	274868.703143	39.512653
2862.014654	275267.917242	39.517671
2864.655721	275687.138164	39.522688
2867.287519	276097.977427	39.527706
2870.362786	276514.309808	39.532724
2873.365568	276932.381065	39.537741
2876.287427	277356.841342	39.542759
2879.110630	277783.273229	39.547776
2882.037643	278214.515236	39.552794
2885.069631	278628.796446	39.557812
2887.897095	279062.213263	39.562829
2891.300927	279472.523216	39.567847
2894.174472	279900.140454	39.572864
2897.190259	280320.647451	39.577882
2900.535982	280754.946834	39.582900
2903.464658	281179.430120	39.587917
2906.395008	281590.220515	39.592935
2909.189995	282021.659576	39.597952
2912.016928	282431.068651	39.602970
2915.306377	282854.884086	39.607988
2918.166841	283288.776000	39.613005
2921.217347	283698.224985	39.618023
2924.196469	284120.843802	39.623040
2927.281918	284550.151859	39.628058
2930.237164	284960.986636	39.633076
2933.096848	285381.565558	39.638093
2936.059914	285802.661161	39.643111
2938.980616	286222.975539	39.648128
2942.162362	286634.585700	39.653146
2945.531309	287055.539488	39.658164
2947.731910	287470.885856	39.663181
2951.190132	287888.217300	39.668199
2954.094182	288307.388753	39.673216
2956.794476	288713.712653	39.678234
2959.674349	289102.123989	39.683252
2962.445237	289481.153038	39.688269
2965.437288	289856.259967	39.693287
2968.165886	290243.855465	39.698304
2971.087821	290622.757497	39.703322
2973.844327	291020.203752	39.708340
2976.276443	291409.140070	39.713357
2979.378866	291809.045243	39.718375
2982.023825	292214.915594	39.723392
2984.841104	292620.173745	39.728410
2987.755169	293028.489598	39.733428
2990.507895	293456.009123	39.738445
2993.502284	293868.019547	39.743463
2996.678052	294307.054003	39.748480
2999.334799	294736.313644	39.753498
3002.421116	295164.615357	39.758516
3004.823394	295612.761963	39.763533
3008.259462	296059.143630	39.768551
3010.975240	296504.520619	39.773568
3014.322288	296957.061660	39.778586
3017.717081	297397.502749	39.783604
3020.855771	297860.464018	39.788621
3024.153979	298304.753936	39.793639
3027.373324	298759.088942	39.798656
3030.793540	299216.642409	39.803674
3034.014131	299654.946428	39.808692
3036.787597	300104.572980	39.813709
3040.114106	300544.813850	39.818727
3043.222269	300996.645747	39.823744
3045.851507	301442.176436	39.828762
3048.976943	301888.719600	39.833780
3051.847950	302352.015746	39.838797
3055.353847	302806.014806	39.843815
3057.978323	303266.045036	39.848832
3061.078903	303723.153581	39.853850
3064.577563	304177.860811	39.858868
3067.359491	304652.035445	39.863885
3070.542838	305108.110445	39.868903
3073.734225	305576.552786	39.873920
3076.770405	306052.282642	39.878938
3080.234207	306502.212477	39.883956
3083.687649	306965.477622	39.888973
3086.769171	307404.822111	39.893991
3089.651278	307865.786827	39.899008
3092.518058	308326.269693	39.904026
3096.004499	308777.635803	39.909044
3099.246301	309255.251688	39.914061
3102.640881	309702.615743	39.919079
3105.782800	310152.024691	39.924096
3108.379535	310612.490842	39.929114
3111.933868	311063.151833	39.934132
3114.838141	311527.756614	39.939149
3117.985368	311982.745514	39.944167
3120.813715	312442.304093	39.949184
3123.742098	312890.745531	39.954202
3126.943636	313311.406195	39.959220
3129.750966	313740.458450	39.964237
3132.866750	314165.955146	39.969255
3136.206573	314586.741326	39.974272
3138.462014	315025.120841	39.979290
3141.595849	315454.927218	39.984308
3144.815636	315884.972181	39.989325
3147.441144	316330.043542	39.994343
3150.241683	316787.631929	39.999360
3153.176245	317238.415726	40.004378
3156.515306	317703.788058	40.009396
3159.213161	318173.120078	40.014413
3162.097430	318647.779222	40.019431
3165.519621	319127.328806	40.024448
3168.454197	319620.007362	40.029466
3171.736182	320102.901183	40.034484
3175.082984	320601.172882	40.039501
3178.213448	321093.888735	40.044519
3181.574375	321598.603539	40.049536
3184.610957	322092.141443	40.054554
3188.101762	322576.487347	40.059572
3191.315573	323094.499251	40.064589
3194.488221	323596.641879	40.069607
3198.008764	324101.545480	40.074624
3200.995695	324610.111307	40.079642
3204.472156	325103.714641	40.084660
3207.866439	325627.929798	40.089677
3210.990178	326131.461667	40.094695
3214.329152	326635.667423	40.099712
3217.401201	327156.317515	40.104730
3220.659826	327672.795287	40.109748
3224.049564	328190.772610	40.114765
3227.310007	328707.268649	40.119783
3230.777908	329231.880038	40.124800
3234.253716	329740.894450	40.129818
3237.515252	330260.528686	40.134836
3240.712379	330764.374448	40.139853
3244.349234	331285.668946	40.144871
3247.404608	331803.242681	40.149888
3250.401314	332318.257274	40.154906
3253.925347	332828.410840	40.159924
3257.420205	333357.203890	40.164941
3260.779813	333861.510250	40.169959
3264.353776	334377.992967	40.174976
3267.376776	334892.679950	40.179994
3270.673382	335411.306404	40.185012
3273.949879	335935.442192	40.190029
3277.390453	336437.558560	40.195047
3281.041645	336959.443415	40.200064
3284.022934	337471.451264	40.205082
3287.592974	337972.926178	40.210100
3290.769733	338484.488959	40.215117
3293.651850	338998.430281	40.220135
3297.218542	339506.647873	40.225152
3300.512716	340010.080323	40.230170
3303.829916	340492.558100	40.235188
3306.917144	340965.978876	40.240205
3309.919671	341423.540731	40.245223
3312.928051	341892.422128	40.250240
3315.731645	342380.552256	40.255258
3319.300458	342866.424755	40.260276
3322.469582	343341.210732	40.265293
3325.336727	343837.545184	40.270311
3328.926585	344331.476233	40.275328
3331.872511	344837.945397	40.280346
3335.167244	345348.188683	40.285364
3338.069281	345854.859128	40.290381
3341.491706	346389.648777	40.295399
3345.090835	346904.120806	40.300416
3348.097661	347437.519333	40.305434
3351.690215	347950.942075	40.310452
3355.130237	348493.528460	40.315469
3358.071380	349024.510609	40.320487
3361.534563	349556.750612	40.325504
3365.008428	350103.707781	40.330522
3368.213473	350646.970267	40.335540
3371.707361	351215.973490	40.340557
3375.183939	351751.718574	40.345575
3378.480067	352306.779552	40.350592
3381.822014	352862.233651	40.355610
3385.421012	353425.738952	40.360628
3388.894966	353982.988038	40.365645
3392.261558	354549.868695	40.370663
3395.870283	355116.044869	40.375680
3399.540415	355684.768818	40.380698
3403.198883	356244.959502	40.385716
3406.337686	356809.718933	40.390733
3409.857629	357365.984707	40.395751
3413.385847	357939.376068	40.400768
3416.369384	358515.613562	40.405786
3420.196740	359074.349753	40.410804
3423.764228	359645.202228	40.415821
3427.350526	360213.456135	40.420839
3431.181293	360772.552952	40.425856
3434.868677	361335.549141	40.430874
3438.394410	361907.498084	40.435892
3441.824094	362471.257559	40.440909
3445.518144	363035.932892	40.445927
3449.384841	363579.737632	40.450944
3452.075305	364139.710773	40.455962
3455.794835	364698.270848	40.460980
3459.149099	365247.009637	40.465997
3462.627059	365833.967097	40.471015
3466.527460	366382.148994	40.476032
3469.657753	366957.219210	40.481050
3473.230843	367513.559795	40.486068
3477.170739	368070.241439	40.491085
3480.349239	368624.194255	40.496103
3484.075480	369175.109834	40.501120
3487.176243	369730.312461	40.506125
3490.269206	370235.252649	40.511130
3493.591788	370684.665525	40.516135
3496.199200	371089.030802	40.521140
3499.023858	371453.442932	40.526144
3501.501420	371769.368125	40.531149
3503.759332	372033.912655	40.536154
3505.626701	372247.715040	40.541159
3507.563340	372429.045011	40.546164
3509.355132	372545.145835	40.551168
3510.353453	372656.512917	40.556173
3511.740689	372709.054153	40.561178
3513.010129	372737.243397	40.566183
3513.340243	372759.272247	40.571188
3514.206439	372730.058550	40.576192
3514.687379	372710.038341	40.581197
3515.398294	372646.481020	40.586202
3515.877451	372576.880298	40.591207
3515.673032	372505.428709	40.596212
3516.185525	372406.109519	40.601216
3516.322472	372301.888808	40.606221
3516.274958	372181.695665	40.611226
3516.724897	372060.609482	40.616231
3516.663291	371938.459043	40.621236
3516.692194	371796.349333	40.626240
3516.443798	371663.644771	40.631245
3516.834304	371511.021252	40.636250
3516.400776	371363.361015	40.641255
3515.994639	371224.599902	40.646260
3515.992551	371059.520394	40.651264
3515.747401	370913.711382	40.656269
3515.403484	370768.248208	40.661274
3515.145041	370618.013699	40.666279
3515.067052	370475.331363	40.671284
3514.772026	370332.021411	40.676288
3514.329041	370193.033818	40.681293
3514.114426	370062.074344	40.686298
3513.927798	369918.949408	40.691303
3513.419583	369798.796952	40.696308
3513.263275	369658.871897	40.701312
3512.856948	369542.467866	40.706317
3512.739155	369411.592882	40.711322
3512.603522	369300.818747	40.716327
3512.181849	369176.173265	40.721332
3512.202728	369055.044672	40.726336
3511.804948	368947.745641	40.731341
3511.857530	368826.458755	40.736346
3511.365375	368730.495492	40.741351
3510.822952	368619.987468	40.746356
3510.796987	368521.329582	40.751360
3510.433534	368438.880205	40.756365
3510.291575	368332.658653	40.761370
3510.356641	368257.341166	40.766375
3510.305086	368173.519020	40.771380
3510.402871	368071.304167	40.776384
3509.849028	367984.406288	40.781389
3509.628287	367893.613860	40.786394
3509.881195	367800.151295	40.791399
3509.447602	367732.010033	40.796404
3509.449637	367632.506148	40.801408
3509.023066	367571.996129	40.806413
3508.735122	367493.578333	40.811418
3508.819497	367421.131324	40.816423
3508.546356	367353.040440	40.821428
3508.428527	367282.075373	40.826432
3508.339951	367227.261390	40.831437
3508.447331	367159.644343	40.836442
3508.343087	367097.072783	40.841447
3507.890550	367040.636915	40.846452
3508.056726	366964.563419	40.851456
3507.992554	366914.350265	40.856461
3507.543106	366861.424735	40.861466
3507.781231	366798.544208	40.866471
3507.649334	366745.746438	40.871476
3507.425170	366679.046121	40.876480
3507.138261	366640.011704	40.881485
3506.907018	366596.007148	40.886490
3507.328825	366545.843967	40.891495
3506.885536	366505.638351	40.896500
3507.026590	366454.399975	40.901504
3506.899460	366413.279245	40.906509
3506.628603	366366.303930	40.911514
3506.280857	366311.733338	40.916519
3506.570899	366283.573230	40.921524
3506.620720	366241.432102	40.926528
3506.307951	366223.315383	40.931533
3506.409429	366173.456854	40.936538
3506.375542	366134.051241	40.941543
3506.149488	366111.162955	40.946548
3506.290791	366067.735059	40.951552
3506.085421	366038.075655	40.956557
3505.973487	365995.349238	40.961562
3505.717442	365973.178025	40.966567
3505.842577	365937.868859	40.971572
3505.925506	365917.374152	40.976576
3505.953344	365890.272968	40.981581
3505.672716	365858.106487	40.986586
3505.942168	365827.125175	40.991591
3505.732397	365796.575802	40.996596
3505.649769	365769.288465	41.001600
3505.384139	365755.972844	41.006605
3505.565120	365723.606078	41.011610
3505.446681	365699.555631	41.016615
3505.381862	365678.041006	41.021620
3505.750673	365659.663654	41.026624
3505.517121	365641.839496	41.031629
3505.378122	365610.515515	41.036634
3505.358120	365584.719312	41.041639
3505.032874	365572.914208	41.046644
3505.350868	365547.751517	41.051648
3505.202227	365536.707224	41.056653
3505.416193	365506.014339	41.061658
3505.475262	365479.467722	41.066663
3504.896742	365458.975602	41.071668
3505.526487	365434.526861	41.076672
3505.213938	365421.752868	41.081677
3504.962508	365406.450325	41.086682
3505.440667	365375.461154	41.091687
3505.149001	365350.572836	41.096692
3505.318768	365342.124262	41.101696
3504.936278	365325.086823	41.106701
3504.988581	365303.120969	41.111706
3505.138140	365279.307809	41.116711
3504.842848	365267.472447	41.121716
3505.069342	365256.852206	41.126720
3504.860093	365243.781955	41.131725
3505.146324	365223.280239	41.136730
3505.327114	365202.540749	41.141735
3504.985978	365176.387987	41.146740
3504.918478	365163.346191	41.151744
3504.821685	365135.475513	41.156749
3504.811590	365128.683713	41.161754
3505.162979	365119.061432	41.166759
3504.460404	365107.010536	41.171764
3504.907365	365077.934352	41.176768
3504.791976	365073.830751	41.181773
3504.813373	365055.228198	41.186778
3505.054452	365039.516908	41.191783
3504.792400	365015.743237	41.196788
3505.077240	365012.466881	41.201792
3504.926594	364989.973203	41.206797
3504.947080	364973.380797	41.211802
3505.059471	364954.229505	41.216807
3504.605008	364930.969634	41.221812
3504.828366	364926.990573	41.226816
3504.992406	364906.431701	41.231821
3504.592181	364890.440088	41.236826
3505.217545	364869.477505	41.241831
3504.718310	364861.770692	41.246836
3504.727888	364839.658707	41.251840
3504.683667	364819.692479	41.256845
3504.815493	364814.557472	41.261850
3504.687553	364796.716287	41.266855
3504.791310	364785.606467	41.271860
3504.768057	364779.223792	41.276864
3504.497880	364757.054219	41.281869
3504.322374	364747.031726	41.286874
3505.023125	364736.565383	41.291879
3504.410222	364722.820929	41.296884
3504.613063	364699.533361	41.301888
3504.517040	364694.434361	41.306893
3504.496310	364683.598633	41.311898
3504.736477	364667.378486	41.316903
3504.394897	364656.389924	41.321908
3504.685989	364653.087111	41.326912
3504.373576	364640.109327	41.331917
3504.311376	364622.817442	41.336922
3504.737106	364618.348375	41.341927
3504.346660	364602.660440	41.346932
3504.687095	364597.034444	41.351936
3504.472459	364586.458340	41.356941
3504.549379	364569.398880	41.361946
3504.733806	364559.522995	41.366951
3504.443984	364545.701969	41.371956
3504.726620	364528.126541	41.376960
3504.558296	364521.079783	41.381965
3504.282784	364513.922749	41.386970
3504.246092	364484.439217	41.391975
3504.601584	364485.604315	41.396980
3504.726348	364469.122461	41.401984
3504.488034	364462.926403	41.406989
3504.528109	364449.409409	41.411994
3504.481684	364433.412593	41.416999
3504.233621	364417.422203	41.422004
3504.219026	364399.181287	41.427008
3504.530157	364406.459918	41.432013
3504.394781	364399.255270	41.437018
3504.206431	364382.237675	41.442023
3504.424141	364392.482562	41.447028
3504.420619	364361.874178	41.452032
3504.107381	364376.604789	41.457037
3504.306828	364350.900416	41.462042
3504.497200	364329.497476	41.467047
3504.217000	364335.113973	41.472052
3504.474532	364318.407525	41.477056
3504.250327	364316.661894	41.482061
3504.309641	364303.599805	41.487066
3504.330670	364290.594653	41.492071
3504.173030	364300.746235	41.497076
3504.279569	364275.972487	41.502080
3504.536094	364265.830702	41.507085
3504.092796	364252.746280	41.512090
3504.537408	364231.633874	41.517095
3504.150193	364241.287439	41.522100
3504.432048	364210.404845	41.527104
3504.542611	364211.659559	41.532109
3504.611761	364195.033734	41.537114
3504.351624	364181.589565	41.542119
3504.330278	364178.615994	41.547124
3504.397681	364164.636605	41.552128
3504.599390	364149.363782	41.557133
3504.291679	364142.491664	41.562138
3504.283506	364126.488694	41.567143
3504.454593	364134.934486	41.572148
3504.285818	364115.343857	41.577152
3504.132737	364112.289331	41.582157
3504.163644	364101.954183	41.587162
3504.157677	364092.057409	41.592167
3504.286836	364087.813283	41.597172
3504.510479	364065.132761	41.602176
3504.053142	364062.609766	41.607181
3504.129705	364049.239551	41.612186
3504.498774	364046.840352	41.617191
3504.146490	364035.064569	41.622196
3504.359261	364026.965171	41.627200
3504.378770	364015.003387	41.632205
3504.261739	364007.719444	41.637210
3504.278299	363993.926150	41.642215
3504.079879	363999.097211	41.647220
3504.785664	363975.958764	41.652224
3504.235386	363979.455255	41.657229
3504.185768	363955.698339	41.662234
3504.573261	363951.209809	41.667239
3504.036290	363933.916388	41.672244
3504.088096	363929.709921	41.677248
3504.205540	363939.436433	41.682253
3504.348923	363911.119938	41.687258
3504.400683	363906.353705	41.692263
3504.415488	363896.479049	41.697268
3504.606788	363875.559190	41.702272
3504.518856	363882.137668	41.707277
3504.270243	363861.312791	41.712282
3504.253454	363855.844954	41.717287
3504.016391	363838.936636	41.722292
3504.263815	363829.355966	41.727296
3504.278593	363828.971964	41.732301
3504.104931	363814.267254	41.737306
3503.868255	363799.292616	41.742311
3504.058397	363808.473336	41.747316
3504.368603	363796.363763	41.752320
3504.017334	363797.538833	41.757325
3503.675010	363788.941931	41.762330
3504.292023	363774.951871	41.767335
3504.319969	363782.962361	41.772340
3504.305246	363756.095639	41.777344
3504.020211	363748.252999	41.782349
3504.314186	363743.728344	41.787354
3504.275216	363727.144888	41.792359
3504.040613	363728.555958	41.797364
3504.376077	363714.712165	41.802368
3504.151053	363706.020372	41.807373
3504.036193	363694.817629	41.812378
3504.180097	363694.056993	41.817383
3504.239774	363689.264043	41.822388
3504.048444	363675.503518	41.827392
3504.043508	363681.051134	41.832397
3504.048392	363662.272519	41.837402
3504.266774	363653.230733	41.842407
3503.861488	363654.363457	41.847412
3504.113768	363629.235547	41.852416
3503.993488	363630.653991	41.857421
3504.157621	363616.252037	41.862426
3504.008447	363621.135468	41.867431
3504.305251	363603.506560	41.872436
3504.332399	363595.716319	41.877440
3503.871341	363600.725390	41.882445
3504.186719	363580.778109	41.887450
3504.082160	363586.723150	41.892455
3503.862093	363583.119404	41.897460
3504.195755	363572.634499	41.902464
3503.971641	363556.894467	41.907469
3504.196921	363558.818060	41.912474
3504.440123	363541.146713	41.917479
3504.108319	363536.135748	41.922484
3504.152784	363509.666634	41.927488
3504.053678	363523.727557	41.932493
3504.226588	363504.845982	41.937498
3504.391121	363503.064309	41.942503
3504.090828	363491.254724	41.947508
3504.083784	363475.429460	41.952512
3504.250779	363476.217275	41.957517
3504.047936	363476.122116	41.962522
3504.163028	363466.104293	41.967527
3503.900749	363442.049957	41.972532
3504.147978	363447.252405	41.977536
3503.858374	363441.293316	41.982541
3503.960841	363426.468498	41.987546
3503.881547	363429.407130	41.992551
3503.910205	363427.519713	41.997556
3504.086064	363420.545597	42.002560
3503.921012	363404.134624	42.007565
3503.576005	363393.935077	42.012570
3503.695865	363397.478337	42.017575
3503.734761	363388.897429	42.022580
3504.055087	363403.655412	42.027584
3504.052006	363395.055696	42.032589
3503.957985	363376.216268	42.037594
3504.291832	363367.970393	42.042599
3503.856423	363382.618856	42.047604
3504.078131	363347.750427	42.052608
3504.347714	363344.908921	42.057613
3503.917991	363354.722056	42.062618
3503.891156	363326.050447	42.067623
3503.828922	363329.597055	42.072628
3504.088693	363321.464660	42.077632
3504.064959	363325.259626	42.082637
3503.842682	363313.666661	42.087642
3503.939541	363296.629023	42.092647
3503.978808	363300.083254	42.097652
3504.311769	363295.068949	42.102656
3504.336263	363286.261298	42.107661
3504.369140	363277.350542	42.112666
3504.436762	363263.040069	42.117671
3503.950153	363250.700098	42.122676
3504.496674	363243.362026	42.127680
3504.200307	363233.790866	42.132685
3503.989983	363225.503770	42.137690
3504.372694	363211.881360	42.142695
3504.118939	363201.998123	42.147700
3503.908940	363181.879282	42.152704
3503.894050	363181.092853	42.157709
3504.043743	363187.939197	42.162714
3504.377110	363174.121020	42.167719
3503.644762	363176.959352	42.172724
3503.900632	363152.059618	42.177728
3503.860705	363162.752619	42.182733
3503.784136	363153.375696	42.187738
3503.679381	363143.239891	42.192743
3503.652211	363140.903287	42.197748
3504.006140	363133.722866	42.202752
3503.701929	363144.228650	42.207757
3503.769615	363145.566505	42.212762
3503.959510	363138.742795	42.217767
3503.718880	363128.501245	42.222772
3503.876999	363118.171211	42.227776
3503.686757	363126.699753	42.232781
3503.922591	363137.196499	42.237786
3504.126857	363127.495284	42.242791
3503.748340	363117.046529	42.247796
3503.959583	363092.993488	42.252800
3504.197975	363098.986153	42.257805
3504.136143	363094.365018	42.262810
3504.073494	363074.604504	42.267815
3503.839238	363081.791452	42.272820
3504.030527	363072.855614	42.277824
3503.913803	363064.477359	42.282829
3503.613019	363046.484709	42.287834
3503.907682	363045.954676	42.292839
3503.571632	363049.900816	42.297844
3503.947435	363054.930315	42.302848
3503.588920	363060.788347	42.307853
3503.525750	363034.259646	42.312858
3504.147155	363027.469481	42.317863
3503.679521	363033.624658	42.322868
3503.719709	363020.565232	42.327872
3504.005105	363030.926943	42.332877
3503.638546	363025.666970	42.337882
3503.951870	363004.422094	42.342887
3503.960019	363002.741458	42.347892
3504.111234	362997.832187	42.352896
3504.294873	362999.228049	42.357901
3504.158334	362986.858111	42.362906
3504.115925	362974.854958	42.367911
3503.896764	362985.627223	42.372916
3504.236516	362958.983893	42.377920
3504.060145	362959.724220	42.382925
3503.925882	362947.684692	42.387930
3504.179622	362938.611733	42.392935
3503.855945	362924.439349	42.397940
3503.729336	362919.701213	42.402944
3503.830826	362922.102405	42.407949
3504.109685	362917.172946	42.412954
3504.030076	362889.094638	42.417959
3503.994089	362905.155897	42.422964
3504.360916	362894.182148	42.427968
3504.333060	362884.695691	42.432973
3504.085588	362875.371175	42.437978
3504.209357	362866.064302	42.442983
3503.954804	362848.573161	42.447988
3503.909241	362835.679907	42.452992
3503.962492	362834.322917	42.457997
3503.854612	362842.151484	42.463002
3504.210714	362815.301930	42.468007
3503.927916	362816.669756	42.473012
3504.008347	362809.405299	42.478016
3503.697574	362805.917611	42.483021
3503.707436	362794.084261	42.488026
3503.924015	362783.363241	42.493031
3503.971648	362786.739853	42.498036
3504.040868	362769.375611	42.503040
3503.921452	362781.455280	42.508045
3503.770386	362767.789900	42.513050
3504.155705	362759.663005	42.518055
3503.761282	362765.755753	42.523060
3503.984837	362753.914056	42.528064
3504.092311	362751.657925	42.533069
3503.775501	362732.751678	42.538074
3504.073577	362726.419701	42.543079
3503.775321	362736.721077	42.548084
3503.990359	362727.705085	42.553088
3503.823583	362718.316891	42.558093
3503.925283	362714.102426	42.563098
3504.027192	362708.310352	42.568103
3503.776287	362707.968342	42.573108
3503.790399	362699.772896	42.578112
3503.713989	362683.856550	42.583117
3503.908713	362681.052283	42.588122
3504.064832	362668.712330	42.593127
3503.902998	362679.551937	42.598132
3504.047541	362657.035902	42.603136
3503.773281	362652.397415	42.608141
3503.713116	362647.139852	42.613146
3504.109406	362650.105129	42.618151
3504.064794	362647.109693	42.623156
3503.710458	362623.960055	42.628160
3503.779565	362634.483271	42.633165
3504.052479	362622.811850	42.638170
3503.988525	362630.226392	42.643175
3503.922831	362610.669722	42.648180
3504.022649	362601.748256	42.653184
3503.968531	362592.367671	42.658189
3503.892699	362592.583213	42.663194
3504.018385	362577.220114	42.668199
3503.466265	362573.439780	42.673204
3503.630736	362557.892429	42.678208
3503.511278	362573.814327	42.683213
3503.198483	362577.171599	42.688218
3503.722593	362565.358675	42.693223
3503.605253	362583.112264	42.698228
3503.955495	362580.257960	42.703232
3503.504083	362567.505127	42.708237
3503.298939	362560.820118	42.713242
3503.651792	362552.749209	42.718247
3503.626902	362552.625916	42.723252
3503.674713	362567.071018	42.728256
3503.951756	362557.332736	42.733261
3503.766927	362562.069245	42.738266
3504.135157	362560.306224	42.743271
3503.734159	362546.756626	42.748276
3503.917672	362526.295400	42.753280
3503.791934	362530.946236	42.758285
3503.918586	362538.686887	42.763290
3504.090049	362519.474360	42.768295
3503.571366	362506.604921	42.773300
3503.812175	362511.452261	42.778304
3504.190183	362515.031113	42.783309
3503.900553	362492.736306	42.788314
3503.674354	362480.787526	42.793319
3503.441526	362478.254397	42.798324
3504.014204	362478.520087	42.803329
3503.967031	362480.664910	42.808333
3503.619987	362492.449855	42.813338
3503.950396	362478.072154	42.818343
3503.668205	362457.735410	42.823348
3503.520997	362457.122555	42.828353
3503.784924	362446.470308	42.833357
3503.824213	362459.339207	42.838362
3503.964453	362449.011852	42.843367
3503.613630	362438.176893	42.848372
3504.141320	362431.019786	42.853377
3503.594408	362431.945923	42.858381
3503.680559	362427.352217	42.863386
3503.966807	362437.052358	42.868391
3503.977787	362432.343311	42.873396
3503.796747	362416.850534	42.878401
3503.718184	362412.384646	42.883405
3503.759465	362405.228094	42.888410
3503.726634	362403.910145	42.893415
3503.476827	362408.835056	42.898420
3504.076757	362407.493409	42.903425
3503.985361	362386.566684	42.908429
3503.999200	362374.376370	42.913434
3504.074711	362379.606085	42.918439
3503.864253	362371.522418	42.923444
3504.014904	362356.129855	42.928449
3503.894845	362367.293714	42.933453
3503.849010	362363.000761	42.938458
3503.800769	362355.425791	42.943463
3503.752631	362336.985809	42.948468
3503.700198	362324.424285	42.953473
3503.706374	362324.474194	42.958477
3503.455472	362341.765534	42.963482
3503.827506	362335.498148	42.968487
3503.813599	362339.520644	42.973492
3503.607791	362330.062208	42.978497
3503.668889	362313.665990	42.983501
3503.600455	362303.931381	42.988506
3503.938316	362302.198597	42.993511
3503.517265	362319.033389	42.998516
3503.699318	362313.381268	43.003521
3504.052877	362306.760568	43.008525
3503.815386	362304.991516	43.013530
3504.098777	362275.557761	43.018535
3503.508725	362278.857105	43.023540
3503.697500	362290.735509	43.028545
3503.569998	362287.982158	43.033549
3503.886893	362287.779387	43.038554
3503.815721	362282.192738	43.043559
3503.524885	362271.806267	43.048564
3503.776858	362257.848018	43.053569
3504.065680	362265.537633	43.058573
3503.456061	362262.580603	43.063578
3503.723295	362265.184632	43.068583
3503.712645	362254.194073	43.073588
3503.938786	362238.433308	43.078593
3503.938515	362240.061826	43.083597
3503.827596	362226.669837	43.088602
3504.174567	362228.141682	43.093607
3503.792491	362225.606688	43.098612
3503.836378	362208.831479	43.103617
3503.643254	362202.831534	43.108621
3503.460890	362201.944339	43.113626
3503.782347	362208.687338	43.118631
3503.410567	362211.341499	43.123636
3503.449492	362210.902776	43.128641
3503.762238	362209.428409	43.133645
3503.495118	362201.531786	43.138650
3504.018618	362181.194778	43.143655
3503.635305	362189.983017	43.148660
3503.646826	362181.304435	43.153665
3503.768520	362173.880686	43.158669
3503.709921	362186.408904	43.163674
3503.831971	362172.776510	43.168679
3503.695856	362156.614974	43.173684
3504.000068	362152.953680	43.178689
3503.953752	362156.319745	43.183693
3503.702503	362152.720818	43.188698
3504.000520	362145.218300	43.193703
3503.677794	362135.905532	43.198708
3503.865690	362134.629016	43.203713
3503.612543	362133.905679	43.208717
3503.566351	362125.745112	43.213722
3503.656545	362133.924160	43.218727
3503.625436	362138.814525	43.223732
3503.926080	362115.993659	43.228737
3503.812708	362106.317003	43.233741
3503.669255	362103.795169	43.238746
3504.045039	362101.293031	43.243751
3503.931845	362100.165892	43.248756
3503.658193	362081.379785	43.253761
3504.065381	362067.829509	43.258765
3504.143899	362068.504110	43.263770
3504.148273	362069.393993	43.268775
3503.745508	362059.152395	43.273780
3503.713344	362054.933588	43.278785
3504.040645	362042.744525	43.283789
3503.795089	362053.826517	43.288794
3503.886389	362042.692567	43.293799
3503.776427	362030.369065	43.298804
3503.674756	362019.341951	43.303809
3503.534449	362021.501518	43.308813
3503.392369	362015.010023	43.313818
3503.701184	362019.490431	43.318823
3503.600893	362021.491002	43.323828
3503.855480	362017.430421	43.328833
3503.794145	362020.875204	43.333837
3503.455102	361999.122323	43.338842
3503.985699	361976.850274	43.343847
3503.711013	361981.677382	43.348852
3503.825788	361994.814371	43.353857
3503.880367	361996.485118	43.358861
3503.760694	361973.679739	43.363866
3503.640914	361967.413718	43.368871
3503.468008	361962.275682	43.373876
3503.649885	361960.669326	43.378881
3503.840549	361965.906327	43.383885
3503.615205	361965.891056	43.388890
3503.739634	361970.069831	43.393895
3503.417108	361971.164066	43.398900
3503.705531	361958.039656	43.403905
3503.746707	361951.671853	43.408909
3503.649620	361954.486164	43.413914
3503.970222	361939.219269	43.418919
3503.412804	361949.765348	43.423924
3503.791108	361948.484171	43.428929
3503.648369	361948.659403	43.433933
3503.462932	361954.948224	43.438938
3503.652617	361923.875128	43.443943
3503.594705	361927.802836	43.448948
3503.697920	361923.180938	43.453953
3503.750533	361922.790939	43.458957
3503.576306	361934.141580	43.463962
3503.628825	361922.555719	43.468967
3503.279128	361930.804344	43.473972
3503.589755	361924.979179	43.478977
3504.101319	361929.656550	43.483981
3503.579537	361915.184392	43.488986
3503.826339	361888.275253	43.493991
3503.566513	361904.601246	43.498996
3503.656750	361898.225679	43.504001
3503.708990	361901.550736	43.509005
3503.782124	361909.121836	43.514010
3503.599745	361887.471362	43.519015
3503.571536	361876.000032	43.524020
3503.704675	361878.319939	43.529025
3503.602825	361874.493811	43.534029
3503.326870	361877.463630	43.539034
3503.581723	361888.746449	43.544039
3503.819305	361883.365395	43.549044
3504.158166	361883.897061	43.554049
3503.897714	361868.416658	43.559053
3504.057780	361852.615319	43.564058
3504.277131	361850.290568	43.569063
3503.878829	361859.742814	43.574068
3504.001398	361830.206980	43.579073
3504.259978	361813.168683	43.584077
3503.988093	361821.939376	43.589082
3503.986934	361804.127890	43.594087
3503.883032	361790.811003	43.599092
3503.805389	361788.100632	43.604097
3504.018672	361785.522385	43.609101
3503.767558	361786.758006	43.614106
3503.961069	361758.076050	43.619111
3503.796298	361757.618634	43.624116
3503.778849	361746.221908	43.629121
3504.056293	361754.142412	43.634125
3503.808307	361747.489506	43.639130
3503.631343	361734.642169	43.644135
3503.839783	361732.471809	43.649140
3503.776886	361733.245107	43.654145
3503.817331	361721.686551	43.659149
3504.079130	361726.225310	43.664154
3504.082414	361705.461432	43.669159
3503.848607	361700.002206	43.674164
3503.722235	361707.503096	43.679169
3504.018470	361695.140738	43.684173
3503.355857	361693.744212	43.689178
3503.636386	361669.272365	43.694183
3503.411224	361672.132386	43.699188
3503.601571	361669.659540	43.704193
3503.365229	361673.081125	43.709197
3503.384497	361677.861793	43.714202
3503.492882	361676.114374	43.719207
3503.529452	361679.874494	43.724212
3503.689209	361680.917937	43.729217
3503.710441	361682.721193	43.734221
3503.644914	361678.660298	43.739226
3503.646793	361669.474240	43.744231
3503.592227	361660.144431	43.749236
3503.426144	361646.557436	43.754241
3503.704570	361654.248794	43.759245
3503.415050	361653.836544	43.764250
3503.735089	361640.681603	43.769255
3503.504741	361655.807091	43.774260
3503.553700	361657.173394	43.779265
3503.888053	361657.603994	43.784269
3503.472864	361652.962242	43.789274
3503.537368	361637.074157	43.794279
3503.264467	361633.529503	43.799284
3503.447455	361624.569258	43.804289
3503.868685	361633.204967	43.809293
3503.498500	361630.922514	43.814298
3503.781565	361628.435009	43.819303
3503.443825	361639.353554	43.824308
3503.574831	361639.867191	43.829313
3503.647547	361632.323873	43.834317
3503.380484	361641.348290	43.839322
3503.244911	361644.524939	43.844327
3502.989163	361652.784205	43.849332
3503.720739	361644.093473	43.854337
3503.555003	361651.397032	43.859341
3503.401120	361659.640194	43.864346
3503.779991	361632.302906	43.869351
3503.529287	361616.540980	43.874356
3503.420374	361624.675257	43.879361
3503.631518	361613.369588	43.884365
3503.725382	361624.805148	43.889370
3503.779526	361613.905979	43.894375
3503.500503	361625.934840	43.899380
3503.575382	361620.783040	43.904385
3503.687115	361623.411687	43.909389
3503.717275	361617.987058	43.914394
3503.965430	361595.326910	43.919399
3503.432754	361604.291543	43.924404
3503.462716	361598.536153	43.929409
3503.792610	361606.982743	43.934413
3503.300587	361607.264084	43.939418
3503.833982	361597.128844	43.944423
3503.548936	361606.944916	43.949428
3503.746989	361598.465746	43.954433
3503.789336	361585.914488	43.959437
3503.559753	361572.795526	43.964442
3503.760159	361573.349083	43.969447
3503.642803	361570.339633	43.974452
3503.435382	361579.074734	43.979457
3503.696469	361572.723005	43.984461
3503.720691	361569.996518	43.989466
3503.965552	361573.113029	43.994471
3503.511720	361562.141481	43.999476
3503.678284	361562.318708	44.004481
3503.599310	361559.735761	44.009485
3503.213891	361567.939205	44.014490
3503.632141	361564.081720	44.019495
3503.737029	361570.782711	44.024500
3503.710002	361572.008357	44.029505
3503.605458	361557.775474	44.034509
3503.493699	361545.655693	44.039514
3503.681907	361529.417226	44.044519
3503.332505	361540.999217	44.049524
3503.709699	361536.359414	44.054529
3503.838814	361533.438225	44.059533
3503.607683	361533.372978	44.064538
3503.819227	361537.207229	44.069543
3503.936751	361529.173350	44.074548
3503.502248	361507.180879	44.079553
3503.401520	361507.324025	44.084557
3503.318161	361498.787544	44.089562
3503.556553	361501.625183	44.094567
3503.255419	361512.512525	44.099572
3503.389330	361511.142745	44.104577
3503.599895	361512.050933	44.109581
3503.490294	361523.747691	44.114586
3503.635417	361509.169979	44.119591
3503.458191	361511.208178	44.124596
3503.366392	361519.237986	44.129601
3503.729185	361516.890543	44.134605
3503.765038	361526.146993	44.139610
3504.384708	361506.863199	44.144615
3503.628592	361490.290543	44.149620
3503.714878	361488.012256	44.154625
3504.227763	361481.239028	44.159629
3503.703761	361475.800207	44.164634
3504.014950	361457.786540	44.169639
3503.772165	361462.150639	44.174644
3503.699747	361461.602284	44.179649
3503.537778	361462.569366	44.184653
3503.475575	361469.220450	44.189658
3503.776874	361452.964079	44.194663
3503.388574	361440.964325	44.199668
3503.300780	361429.069735	44.204673
3503.590467	361418.438630	44.209677
3503.493242	361424.611794	44.214682
3503.612060	361429.732985	44.219687
3503.327266	361434.129174	44.224692
3503.751218	361425.410698	44.229697
3503.756224	361431.644035	44.234701
3503.713645	361433.126598	44.239706
3503.818910	361435.476378	44.244711
3503.601099	361415.230789	44.249716
3503.576242	361407.499297	44.254721
3503.851479	361409.313299	44.259725
3503.830492	361410.207204	44.264730
3503.878530	361402.260624	44.269735
3503.345695	361407.688400	44.274740
3503.395612	361412.642367	44.279745
3503.692608	361418.651428	44.284749
3503.273339	361396.885507	44.289754
3503.824716	361385.958570	44.294759
3503.389027	361372.694017	44.299764
3503.475184	361382.578680	44.304769
3503.415038	361384.852831	44.309773
3503.507687	361383.642243	44.314778
3503.648842	361380.744586	44.319783
3503.425256	361391.925041	44.324788
3503.640184	361389.371959	44.329793
3503.697375	361390.864196	44.334797
3503.313169	361396.599267	44.339802
3503.880158	361396.662302	44.344807
3503.679428	361383.920408	44.349812
3503.648153	361370.795486	44.354817
3503.541209	361367.758932	44.359821
3503.539984	361365.163683	44.364826
3503.674134	361355.244180	44.369831
3503.645413	361376.673806	44.374836
3503.613974	361358.129021	44.379841
3503.763589	361368.868801	44.384845
3503.530182	361365.954021	44.389850
3503.996774	361347.432281	44.394855
3503.635773	361336.904023	44.399860
3503.608612	361340.852364	44.404865
3503.815729	361335.018045	44.409869
3503.595312	361334.467640	44.414874
3503.798813	361334.740811	44.419879
3503.585376	361332.433563	44.424884
3503.502852	361323.260781	44.429889
3503.582475	361307.141186	44.434893
3503.064878	361314.678540	44.439898
3503.729746	361321.392823	44.444903
3503.513599	361313.742447	44.449908
3503.779853	361313.420451	44.454913
3503.710681	361309.843566	44.459917
3503.444353	361310.827149	44.464922
3503.150090	361323.901761	44.469927
3503.611018	361324.668591	44.474932
3503.966137	361313.161971	44.479937
3504.081114	361292.609265	44.484941
3503.675659	361292.113557	44.489946
3503.720263	361290.630661	44.494951
3503.394294	361286.865361	44.499956
3503.266670	361284.926228	44.504961
3503.636645	361290.592976	44.509965
3503.561204	361294.625290	44.514970
3503.786942	361287.032281	44.519975
3503.549721	361279.817805	44.524980
3503.499565	361270.105540	44.529985
3503.646262	361256.290867	44.534989
3503.575404	361269.126612	44.539994
3503.827785	361261.478497	44.544999
3503.618296	361265.786459	44.550004
3503.576860	361268.057657	44.555009
3503.847268	361270.890249	44.560013
3503.450447	361252.275958	44.565018
3503.974420	361233.108964	44.570023
3503.438570	361241.845156	44.575028
3503.659603	361231.301199	44.580033
3503.663520	361233.514338	44.585037
3503.436645	361241.489210	44.590042
3503.637697	361234.765244	44.595047
3503.685522	361234.070650	44.600052
3503.363329	361235.292075	44.605057
3503.423152	361233.425089	44.610061
3503.562337	361224.064565	44.615066
3503.786091	361206.878883	44.620071
3503.705412	361208.138466	44.625076
3503.636707	361204.485162	44.630081
3503.547608	361206.534888	44.635085
3503.622870	361208.991205	44.640090
3503.771153	361209.782017	44.645095
3503.665108	361216.719969	44.650100
3503.883799	361208.466477	44.655105
3503.771926	361185.812160	44.660109
3503.574817	361181.441232	44.665114
3503.633909	361176.902574	44.670119
3503.608497	361195.838092	44.675124
3503.715671	361183.327370	44.680129
3503.846064	361186.029429	44.685133
3503.593274	361181.616412	44.690138
3503.627565	361162.374129	44.695143
3503.594306	361162.964631	44.700148
3503.668966	361150.586269	44.705153
3503.723235	361166.582959	44.710157
3503.839303	361172.722436	44.715162
3503.924903	361160.774922	44.720167
3503.825373	361137.686056	44.725172
3503.626843	361121.610371	44.730177
3503.734699	361124.443223	44.735181
3503.443446	361129.807394	44.740186
3503.324617	361123.362992	44.745191
3503.465076	361132.857438	44.750196
3503.877716	361137.499636	44.755201
3503.892732	361133.604081	44.760205
3503.584750	361123.372742	44.765210
3503.684153	361098.700226	44.770215
3503.626964	361104.052842	44.775220
3503.643521	361095.933069	44.780225
3503.785215	361099.778398	44.785229
3503.481672	361092.269032	44.790234
3503.562289	361102.358193	44.795239
3503.763421	361101.181340	44.800244
3503.857631	361090.046706	44.805249
3503.859199	361077.552652	44.810253
3503.375467	361076.611295	44.815258
3504.105594	361070.745154	44.820263
3503.752201	361077.035196	44.825268
3503.765816	361055.735043	44.830273
3503.741735	361036.120252	44.835277
3503.583937	361040.216498	44.840282
3503.474561	361037.714666	44.845287
3503.675757	361042.110398	44.850292
3503.446046	361041.154328	44.855297
3503.789268	361038.224706	44.860301
3503.693159	361041.446047	44.865306
3503.792569	361036.290306	44.870311
3503.808268	361021.911025	44.875316
3503.859716	361006.279250	44.880321
3503.707314	361006.608687	44.885325
3503.506662	361010.126460	44.890330
3503.759379	361007.007578	44.895335
3503.706973	361005.743575	44.900340
3503.665485	360998.014646	44.905345
3503.625398	360976.824730	44.910349
3503.653268	360988.728898	44.915354
3503.686816	360971.242408	44.920359
3503.650613	360981.960759	44.925364
3503.555760	360981.390499	44.930369
3503.517398	360979.004666	44.935373
3503.361130	360988.342484	44.940378
3503.580013	360978.536736	44.945383
3503.644653	360980.078700	44.950388
3503.572410	360962.888833	44.955393
3503.859819	360941.850693	44.960397
3503.625642	360955.221256	44.965402
3504.057015	360943.448036	44.970407
3503.532635	360953.073066	44.975412
3503.640964	360946.999860	44.980417
3503.840785	360937.731477	44.985421
3503.536154	360923.682710	44.990426
3503.725363	360922.304171	44.995431
3503.468064	360918.426203	45.000436
3503.567394	360915.280673	45.005441
3503.658128	360919.490313	45.010445
3503.316210	360926.033019	45.015450
3503.776888	360913.949810	45.020455
3503.474578	360929.137796	45.025460
3503.603461	360913.341076	45.030465
3503.647606	360905.624040	45.035469
3503.649928	360886.946506	45.040474
3503.805965	360894.886347	45.045479
3503.544604	360891.492488	45.050484
3503.741010	360880.468878	45.055489
3503.860745	360890.501009	45.060493
3503.472289	360895.117200	45.065498
3503.676664	360868.239638	45.070503
3503.645296	360879.822403	45.075508
3503.278659	360856.419387	45.080513
3503.526117	360853.708459	45.085517
3503.293110	360845.780771	45.090522
3503.529626	360863.428171	45.095527
3503.312149	360855.905161	45.100532
3503.433293	360863.799632	45.105537
3503.478988	360858.143448	45.110541
3503.114960	360871.101984	45.115546
3503.719584	360860.751762	45.120551
3503.476873	360876.973618	45.125556
3503.447098	360868.504890	45.130561
3503.720265	360876.604338	45.135565
3503.647217	360875.750727	45.140570
3503.539556	360878.210533	45.145575
3503.216951	360873.757633	45.150580
3503.755472	360865.300847	45.155585
3503.687159	360847.194270	45.160589
3503.512990	360849.639146	45.165594
3503.758605	360844.053139	45.170599
3503.678091	360845.694392	45.175604
3503.570862	360848.128686	45.180609
3503.632617	360845.854247	45.185613
3503.596640	360844.892991	45.190618
3503.365855	360845.565615	45.195623
3503.359082	360839.408809	45.200628
3503.394792	360845.103009	45.205633
3503.648988	360813.917207	45.210637
3503.064435	360824.009800	45.215642
3503.469622	360810.968399	45.220647
3503.440378	360820.591519	45.225652
3503.494452	360815.468367	45.230657
3503.365846	360816.277512	45.235661
3503.521305	360813.123102	45.240666
3503.444835	360814.305692	45.245671
3503.335973	360819.844630	45.250676
3503.435897	360835.325298	45.255681
3503.433487	360823.188046	45.260685
3503.000574	360823.358263	45.265690
3503.317176	360821.705125	45.270695
3503.541214	360829.914130	45.275700
3503.440012	360828.886849	45.280705
3503.701743	360838.565748	45.285709
3503.774964	360840.335371	45.290714
3503.961708	360839.542472	45.295719
3503.629880	360836.465098	45.300724
3503.673481	360812.564629	45.305729
3503.948498	360799.594695	45.310733
3503.724290	360809.197746	45.315738
3503.687793	360814.063654	45.320743
3503.615329	360815.474622	45.325748
3503.541012	360807.725407	45.330753
3503.608584	360808.605322	45.335757
3503.433153	360782.729248	45.340762
3503.710395	360772.685221	45.345767
3503.610315	360780.665570	45.350772
3503.382393	360778.258802	45.355777
3503.807694	360776.944719	45.360781
3503.570289	360770.010099	45.365786
3503.691152	360772.662796	45.370791
3503.559610	360774.770141	45.375796
3503.478781	360778.777904	45.380801
3503.444099	360790.971914	45.385805
3503.606557	360765.245980	45.390810
3503.985976	360758.493750	45.395815
3503.753991	360743.975421	45.400820
3503.569913	360756.396623	45.405825
3503.757893	360739.241875	45.410829
3503.512145	360751.876394	45.415834
3503.575678	360757.617097	45.420839
3503.298528	360757.991703	45.425844
3503.634046	360750.355808	45.430849
3503.820103	360732.336204	45.435853
3503.495110	360742.209660	45.440858
3503.873869	360732.047792	45.445863
3503.634907	360736.920269	45.450868
3503.673950	360736.303393	45.455873
3503.714332	360726.729379	45.460877
3503.464978	360720.890811	45.465882
3503.513327	360708.694615	45.470887
3503.646935	360702.744611	45.475892
3503.535078	360705.892127	45.480897
3503.580121	360695.553995	45.485901
3503.455780	360713.207606	45.490906
3504.179146	360682.939937	45.495911
3503.522500	360700.219678	45.500916
3503.693273	360702.839043	45.505921
3503.916847	360695.373512	45.510925
3503.380941	360677.111780	45.515930
3503.266651	360668.198352	45.520935
3503.614773	360666.031309	45.525940
3503.724095	360671.052299	45.530945
3503.861912	360672.582704	45.535949
3503.865175	360685.864913	45.540954
3504.007471	360671.160163	45.545959
3503.641986	360662.388229	45.550964
3503.432353	360642.980732	45.555969
3503.701612	360635.584307	45.560973
3503.506789	360635.309751	45.565978
3503.726680	360629.015302	45.570983
3503.644920	360645.771601	45.575988
3503.536930	360637.391535	45.580993
3503.666763	360644.088713	45.585997
3503.313984	360643.152090	45.591002
3503.537288	360623.498022	45.596007
3503.452175	360623.918607	45.601012
3503.173491	360614.649470	45.606017
3503.636408	360613.660232	45.611021
3503.527065	360603.550054	45.616026
3503.357076	360605.332689	45.621031
3503.305326	360615.671892	45.626036
3503.509312	360605.130493	45.631041
3503.277705	360614.607523	45.636045
3502.790330	360606.592779	45.641050
3503.580267	360614.661467	45.646055
3503.326173	360616.635518	45.651060
3503.304866	360615.493818	45.656065
3503.680901	360625.205582	45.661069
3503.555471	360631.281524	45.666074
3503.578773	360624.280222	45.671079
3503.597233	360622.725101	45.676084
3503.843856	360625.688721	45.681089
3504.250641	360617.787081	45.686093
3503.558958	360606.267658	45.691098
3503.453428	360590.380659	45.696103
3503.648432	360590.298936	45.701108
3503.651248	360585.361984	45.706113
3503.790892	360592.312077	45.711117
3503.734596	360580.564971	45.716122
3503.890770	360582.626841	45.721127
3503.712252	360563.316176	45.726132
3503.350351	360563.602397	45.731137
3503.609824	360547.097872	45.736141
3503.285879	360569.872273	45.741146
3503.272810	360554.988481	45.746151
3503.376765	360561.842437	45.751156
3503.361320	360559.376622	45.756161
3503.775362	360565.672638	45.761165
3503.785995	360573.457398	45.766170
3503.694917	360562.759069	45.771175
3503.579776	360572.141358	45.776180
3503.611880	360559.362436	45.781185
3503.912678	360538.194774	45.786189
3503.389591	360535.783764	45.791194
3503.575833	360525.041585	45.796199
3503.738257	360532.751463	45.801204
3503.539138	360533.317301	45.806209
3503.895004	360526.975897	45.811213
3503.801916	360536.329261	45.816218
3503.991114	360518.588985	45.821223
3503.740508	360500.791002	45.826228
3503.223168	360504.791457	45.831233
3503.734903	360507.942187	45.836237
3503.682690	360502.606791	45.841242
3503.742493	360508.958815	45.846247
3503.715810	360503.364924	45.851252
3503.665396	360477.036341	45.856257
3503.721892	360467.612404	45.861261
3503.499154	360471.210045	45.866266
3503.707011	360453.543134	45.871271
3503.415419	360460.052500	45.876276
3503.715589	360463.771044	45.881281
3504.005986	360461.511333	45.886285
3503.749770	360454.732317	45.891290
3503.216398	360440.821353	45.896295
3503.191705	360430.952216	45.901300
3503.160936	360432.178482	45.906305
3503.489836	360432.050145	45.911309
3503.208991	360435.504299	45.916314
3503.360472	360430.187586	45.921319
3503.416945	360437.176296	45.926324
3503.067174	360439.241817	45.931329
3503.360190	360427.973818	45.936333
3502.991719	360446.404054	45.941338
3503.326294	360460.982585	45.946343
3503.740516	360465.115679	45.951348
3503.338447	360448.155891	45.956353
3503.522191	360445.607689	45.961357
3503.545184	360452.932487	45.966362
3503.705157	360443.568524	45.971367
3503.526945	360446.472087	45.976372
3503.358737	360458.152925	45.981377
3503.506219	360441.258932	45.986381
3503.251158	360459.187761	45.991386
3503.392891	360449.114197	45.996391
3503.443153	360454.806142	46.001396
3503.278098	360462.338788	46.006401
3503.320501	360456.632186	46.011405
3503.409181	360464.582747	46.016410
3503.706859	360457.588937	46.021415
3503.568074	360458.705050	46.026420
3503.356772	360470.799832	46.031425
3503.595990	360464.196954	46.036429
3503.428936	360462.162237	46.041434
3503.797920	360443.502904	46.046439
3503.660410	360432.608318	46.051444
3503.467956	360433.783807	46.056449
3503.625805	360433.936970	46.061453
3503.444401	360439.156622	46.066458
3503.459572	360429.357520	46.071463
3503.688708	360436.140813	46.076468
3503.612053	360437.603347	46.081473
3503.825040	360431.691653	46.086477
3503.600523	360419.716642	46.091482
3503.543274	360406.264764	46.096487
3503.343773	360411.818076	46.101492
3503.398384	360408.399677	46.106497
3503.736384	360397.633479	46.111501
3503.871396	360410.971273	46.116506
3503.861903	360411.456243	46.121511
3503.920554	360398.138716	46.126516
3503.383296	360385.704218	46.131521
3503.750357	360373.737458	46.136525
3503.374674	360373.491493	46.141530
3503.621307	360359.431749	46.146535
3503.499743	360384.846074	46.151540
3503.800142	360368.691262	46.156545
3504.001883	360371.000397	46.161549
3503.694738	360372.728385	46.166554
3503.627451	360355.588409	46.171559
3503.702396	360345.296366	46.176564
3504.043841	360336.870644	46.181569
3503.657110	360331.944356	46.186573
3503.430660	360341.166165	46.191578
3503.525084	360332.855830	46.196583
3503.574669	360337.682731	46.201588
3503.715904	360332.774763	46.206593
3503.667124	360315.937200	46.211597
3503.574615	360310.557261	46.216602
3503.673604	360306.037659	46.221607
3503.551328	360307.965438	46.226612
3503.131649	360313.909814	46.231617
3503.677682	360313.594474	46.236621
3503.360178	360317.792367	46.241626
3503.527828	360314.432429	46.246631
3503.292075	360311.925091	46.251636
3503.359781	360310.082269	46.256641
3503.445945	360306.099061	46.261645
3503.332824	360309.272249	46.266650
3503.671194	360310.541946	46.271655
3503.472508	360318.639744	46.276660
3503.424772	360317.858459	46.281665
3503.717822	360309.058692	46.286669
3503.403780	360292.263054	46.291674
3503.351710	360290.490059	46.296679
3503.571850	360292.007462	46.301684
3503.361685	360287.892976	46.306689
3503.482198	360282.886495	46.311693
3503.119287	360292.893267	46.316698
3503.227369	360294.123033	46.321703
3503.772886	360288.922133	46.326708
3503.416093	360299.106060	46.331713
3503.421865	360292.209265	46.336717
3503.420394	360291.878695	46.341722
3503.656181	360291.103480	46.346727
3503.835660	360295.019239	46.351732
3503.734503	360292.032593	46.356737
3503.734665	360291.116506	46.361741
3503.605881	360273.299179	46.366746
3503.480520	360261.003101	46.371751
3503.479892	360251.206461	46.376756
3503.425997	360266.686183	46.381761
3503.415709	360263.965077	46.386765
3503.227942	360260.559538	46.391770
3503.423417	360269.841889	46.396775
3503.182873	360272.704425	46.401780
3503.367641	360268.603841	46.406785
3503.726220	360264.450335	46.411789
3503.391467	360268.956311	46.416794
3503.385871	360266.056341	46.421799
3503.324643	360276.269885	46.426804
3503.562416	360271.855570	46.431809
3503.620736	360268.487466	46.436813
3503.647486	360268.228773	46.441818
3504.065974	360258.340431	46.446823
3503.496097	360249.346272	46.451828
3503.536277	360235.039223	46.456833
3503.418029	360241.572108	46.461837
3503.306138	360237.213067	46.466842
3503.356899	360242.777729	46.471847
3503.580868	360241.011984	46.476852
3503.360348	360251.327054	46.481857
3503.661155	360246.521081	46.486861
3503.565165	360254.602655	46.491866
3503.753709	360240.373938	46.496871
3503.445037	360249.456086	46.501876
3503.242185	360248.750214	46.506881
3504.117097	360232.631763	46.511885
3503.569849	360224.626419	46.516890
3503.664664	360217.613753	46.521895
3503.564934	360209.944796	46.526900
3503.616779	360215.127598	46.531905
3503.623660	360206.551174	46.536909
3503.523257	360223.208783	46.541914
3503.785607	360211.792904	46.546919
3503.571531	360200.376002	46.551924
3503.298929	360194.490152	46.556929
3503.825773	360181.047657	46.561933
3503.519233	360184.378661	46.566938
3503.380578	360183.408178	46.571943
3503.804312	360192.654459	46.576948
3503.798082	360190.085384	46.581953
3503.772071	360183.473506	46.586957
3503.383256	360194.934821	46.591962
3503.771193	360177.163002	46.596967
3503.860538	360157.020999	46.601972
3503.256970	360163.172587	46.606977
3503.442775	360148.053661	46.611981
3503.844306	360157.557921	46.616986
3503.500321	360157.154266	46.621991
3503.519394	360155.929833	46.626996
3503.633751	360151.433234	46.632001
3503.802667	360160.643466	46.637005
3503.201516	360142.977105	46.642010
3503.458086	360127.719756	46.647015
3503.547441	360123.939598	46.652020
3503.201710	360121.144282	46.657025
3503.652392	360119.164570	46.662029
3503.737620	360118.489493	46.667034
3503.616045	360122.503752	46.672039
3503.630150	360120.618504	46.677044
3503.295360	360130.849879	46.682049
3503.568780	360117.778230	46.687053
3503.517295	360128.346511	46.692058
3503.501081	360123.895996	46.697063
3503.395655	360135.566987	46.702068
3503.152956	360127.208127	46.707073
3503.455455	360130.544637	46.712077
3503.320795	360139.268497	46.717082
3503.284511	360134.363126	46.722087
3503.687848	360147.429560	46.727092
3503.415400	360133.121011	46.732097
3503.568744	360104.826107	46.737101
3503.510073	360115.573650	46.742106
3503.648169	360097.154252	46.747111
3503.705203	360089.435048	46.752116
3503.686934	360106.995774	46.757121
3503.634204	360096.774755	46.762125
3503.517493	360104.757845	46.767130
3503.613976	360104.666250	46.772135
3503.566824	360106.149576	46.777140
3503.711531	360094.090668	46.782145
3503.679450	360077.148596	46.787149
3503.365726	360085.697204	46.792154
3503.712086	360070.451088	46.797159
3503.358307	360062.211562	46.802164
3503.422080	360079.555759	46.807169
3503.552693	360076.252552	46.812173
3503.118812	360084.820156	46.817178
3503.550608	360084.370197	46.822183
3503.426592	360077.595675	46.827188
3503.441919	360077.007986	46.832193
3503.599125	360073.726020	46.837197
3503.654652	360077.737731	46.842202
3503.846506	360066.053055	46.847207
3503.858056	360050.401831	46.852212
3503.336785	360050.280664	46.857217
3503.710381	360043.529255	46.862221
3503.819386	360038.320998	46.867226
3503.842672	360033.864231	46.872231
3503.653036	360036.438824	46.877236
3503.289467	360017.208087	46.882241
3503.670097	360007.987280	46.887245
3503.548173	360006.861472	46.892250
3503.594381	360009.246105	46.897255
3503.605072	360005.605605	46.902260
3503.785103	360003.643229	46.907265
3503.814101	360008.168063	46.912269
3503.455800	360007.410424	46.917274
3504.039140	360006.631153	46.922279
3503.398456	359983.983529	46.927284
3503.329599	359978.039997	46.932289
3503.758489	359971.915992	46.937293
3503.575274	359969.171314	46.942298
3503.832249	359970.937366	46.947303
3503.562160	359980.140696	46.952308
3503.400452	359979.453762	46.957313
3503.422356	359975.200778	46.962317
3503.471290	359980.384065	46.967322
3503.719209	359968.156132	46.972327
3503.659530	359975.392287	46.977332
3503.547982	359956.656055	46.982337
3503.763685	359944.738563	46.987341
3503.689328	359950.908301	46.992346
3503.720092	359937.009792	46.997351
3503.914731	359944.409317	47.002356
3503.960522	359936.717312	47.007361
3503.847873	359910.830844	47.012365
3503.554290	359911.538854	47.017370
3503.859905	359901.337483	47.022375
3503.393429	359912.047755	47.027380
3503.296527	359907.024713	47.032385
3503.673702	359915.006095	47.037389
3503.414272	359916.879233	47.042394
3503.116145	359913.134869	47.047399
3503.266383	359909.701317	47.052404
3503.294041	359915.625915	47.057409
3503.470520	359912.748033	47.062413
3503.302164	359916.464349	47.067418
3503.591753	359905.349447	47.072423
3503.389523	359913.778674	47.077428
3503.196885	359915.234114	47.082433
3503.741288	359912.348959	47.087437
3503.553781	359912.327705	47.092442
3503.431839	359891.073912	47.097447
3503.399515	359883.317909	47.102452
3503.237556	359888.051066	47.107457
3503.137790	359881.069112	47.112461
3502.953095	359896.315169	47.117466
3503.406978	359908.381272	47.122471
3503.652601	359914.118736	47.127476
3502.976109	359902.265941	47.132481
3503.299998	359907.838355	47.137485
3503.136365	359927.076132	47.142490
3503.371176	359922.738593	47.147495
3503.623649	359923.767417	47.152500
3503.489445	359923.610505	47.157505
3503.588437	359898.301283	47.162509
3503.357249	359894.546335	47.167514
3503.497341	359896.407206	47.172519
3503.656260	359888.010261	47.177524
3503.301942	359896.336303	47.182529
3503.643284	359893.101555	47.187533
3503.395903	359896.245102	47.192538
3503.495972	359894.498933	47.197543
3503.523584	359897.344544	47.202548
3503.565164	359902.961588	47.207553
3503.248822	359897.209848	47.212557
3503.036461	359919.101743	47.217562
3503.243179	359897.490640	47.222567
3503.758336	359908.681885	47.227572
3503.323131	359911.066290	47.232577
3503.557397	359903.777070	47.237581
3503.219407	359910.039383	47.242586
3503.165595	359915.315258	47.247591
3503.573884	359908.278437	47.252596
3503.577880	359905.962192	47.257601
3503.665472	359899.815795	47.262605
3503.725537	359886.243440	47.267610
3503.404214	359876.700993	47.272615
3503.438415	359879.011192	47.277620
3503.202306	359880.193595	47.282625
3503.478082	359878.037954	47.287629
3503.441429	359876.211613	47.292634
3503.287374	359875.269006	47.297639
3503.404763	359882.553521	47.302644
3503.494790	359877.755387	47.307649
3503.491504	359877.654117	47.312653
3503.253220	359885.910925	47.317658
3503.589480	359879.038164	47.322663
3503.761537	359880.970322	47.327668
3503.383880	359884.974191	47.332673
3503.493478	359883.277408	47.337677
3503.575258	359888.455512	47.342682
3503.266162	359893.771747	47.347687
3503.628512	359895.241235	47.352692
3503.392280	359894.718759	47.357697
3503.869075	359874.591726	47.362701
3503.204694	359867.062872	47.367706
3503.393255	359867.923678	47.372711
3503.292957	359876.235013	47.377716
3503.241937	359874.131034	47.382721
3503.140760	359874.325149	47.387725
3503.386480	359883.065260	47.392730
3503.269406	359875.220868	47.397735
3503.682980	359871.516667	47.402740
3503.543295	359872.734720	47.407745
3503.637203	359869.615425	47.412749
3503.616078	359878.906647	47.417754
3503.532396	359876.527923	47.422759
3503.632908	359888.599004	47.427764
3503.033531	359877.064812	47.432769
3503.193466	359875.945335	47.437773
3503.120421	359895.245143	47.442778
3503.306990	359880.227798	47.447783
3503.295969	359893.105343	47.452788
3502.914428	359888.508991	47.457793
3503.476301	359891.906299	47.462797
3503.394511	359898.000879	47.467802
3503.518988	359897.065132	47.472807
3503.737673	359879.370853	47.477812
3503.552361	359902.479899	47.482817
3503.713850	359890.189271	47.487821
3503.747135	359892.626845	47.492826
3503.713877	359864.870225	47.497831
3503.714367	359864.717466	47.502836
3503.603463	359862.012243	47.507841
3503.752071	359848.451327	47.512845
3503.768172	359856.769710	47.517850
3503.596015	359851.758559	47.522855
3503.540442	359851.512878	47.527860
3503.290716	359834.274327	47.532865
3503.415696	359822.498379	47.537869
3503.110278	359817.202935	47.542874
3503.388432	359817.744223	47.547879
3503.360380	359818.003117	47.552884
3503.358452	359829.072554	47.557889
3503.727263	359811.303625	47.562893
3503.687252	359827.162987	47.567898
3503.689320	359819.579661	47.572903
3503.742982	359813.820310	47.577908
3503.507180	359829.023575	47.582913
3503.575142	359821.124476	47.587917
3503.595938	359833.666205	47.592922
3503.732866	359813.236628	47.597927
3503.480162	359798.619503	47.602932
3503.675636	359795.306023	47.607937
3503.826671	359781.846490	47.612941
3503.260549	359791.732813	47.617946
3503.385489	359791.356809	47.622951
3503.671883	359795.790080	47.627956
3503.420460	359788.679410	47.632961
3503.672021	359789.199455	47.637965
3503.518940	359791.819175	47.642970
3503.365263	359791.563556	47.647975
3503.706471	359796.089946	47.652980
3503.522346	359795.355661	47.657985
3503.947584	359767.679180	47.662989
3503.636921	359778.517527	47.667994
3503.480533	359762.841866	47.672999
3503.703936	359766.343584	47.678004
3503.808810	359767.395746	47.683009
3503.399335	359764.177899	47.688013
3503.213224	359772.121123	47.693018
3503.266979	359770.000576	47.698023
3503.499955	359766.553934	47.703028
3503.271999	359774.910913	47.708033
3503.527985	359769.984747	47.713037
3503.465379	359777.246841	47.718042
3503.480277	359760.933390	47.723047
3503.552941	359745.908564	47.728052
3503.376055	359734.205763	47.733057
3503.890555	359726.236056	47.738061
3503.563203	359735.906519	47.743066
3503.823962	359738.867960	47.748071
3503.670557	359735.049810	47.753076
3503.535602	359735.401943	47.758081
3503.766202	359739.335112	47.763085
3503.473785	359719.380511	47.768090
3503.562543	359710.205790	47.773095
3503.565427	359707.686141	47.778100
3503.440613	359703.379988	47.783105
3503.846296	359703.443082	47.788109
3503.379588	359706.315957	47.793114
3503.842482	359693.392365	47.798119
3503.981638	359696.042229	47.803124
3503.652081	359699.605921	47.808129
3503.793708	359672.686721	47.813133
3503.615298	359670.221176	47.818138
3503.409669	359659.235399	47.823143
3503.514740	359663.137526	47.828148
3503.626005	359660.804312	47.833153
3503.343955	359665.454691	47.838157
3503.168255	359665.813266	47.843162
3503.588396	359659.716051	47.848167
3503.542681	359670.359858	47.853172
3503.382271	359669.596375	47.858177
3503.660593	359669.883175	47.863181
3503.481695	359663.117270	47.868186
3503.018185	359665.557054	47.873191
3503.440010	359668.874732	47.878196
3503.546757	359673.387307	47.883201
3503.824709	359666.676412	47.888205
3503.559959	359647.633477	47.893210
3503.412752	359634.424622	47.898215
3503.540199	359629.620548	47.903220
3503.364482	359642.600536	47.908225
3503.724665	359639.795381	47.913229
3503.409400	359647.530025	47.918234
3503.248536	359639.896089	47.923239
3503.385381	359639.747219	47.928244
3503.418129	359640.479983	47.933249
3504.013341	359645.017126	47.938253
3503.103783	359653.710897	47.943258
3503.513433	359652.170241	47.948263
3503.616169	359647.013826	47.953268
3503.547009	359639.009143	47.958273
3503.387177	359618.473720	47.963277
3503.455190	359615.536628	47.968282
3503.553414	359605.876908	47.973287
3503.426115	359602.818013	47.978292
3503.584026	359603.505544	47.983297
3503.746902	359602.970863	47.988301
3503.489382	359602.578981	47.993306
3503.516566	359607.333157	47.998311
3503.684860	359620.004303	48.003316
3503.392723	359623.562085	48.008321
3503.539777	359616.133931	48.013325
3503.257816	359622.540101	48.018330
3503.199241	359613.617671	48.023335
3503.129117	359615.893482	48.028340
3503.520700	359620.310139	48.033345
3503.603239	359611.110936	48.038349
3503.175519	359623.570946	48.043354
3503.354470	359621.354261	48.048359
3503.050620	359613.055873	48.053364
3502.920122	359623.662201	48.058369
3503.427494	359617.042263	48.063373
3503.292653	359625.409994	48.068378
3503.304036	359625.128280	48.073383
3503.473618	359618.841653	48.078388
3503.058267	359634.607737	48.083393
3503.649121	359618.661221	48.088397
3503.424869	359635.262272	48.093402
3503.508768	359624.001698	48.098407
3503.619080	359627.521304	48.103412
3503.406711	359622.338361	48.108417
3503.319882	359600.162820	48.113421
3503.232514	359599.591360	48.118426
3503.237477	359604.628960	48.123431
3503.661458	359611.610583	48.128436
3503.261840	359604.167064	48.133441
3503.647824	359592.502477	48.138445
3503.554519	359607.225248	48.143450
3503.534190	359603.971318	48.148455
3503.658723	359609.880639	48.153460
3503.738575	359609.791672	48.158465
3503.413553	359603.964930	48.163469
3503.760162	359611.645838	48.168474
3503.729657	359605.543519	48.173479
3503.468034	359599.401397	48.178484
3503.273610	359591.594634	48.183489
3503.474403	359568.253966	48.188493
3503.518553	359569.977339	48.193498
3503.543099	359576.207829	48.198503
3503.460476	359572.225798	48.203508
3503.405760	359570.682211	48.208513
3503.589987	359573.070493	48.213517
3503.453365	359571.539856	48.218522
3503.557225	359562.159147	48.223527
3503.456368	359569.427319	48.228532
3503.146537	359567.669599	48.233537
3503.652529	359571.330228	48.238541
3503.561348	359571.497317	48.243546
3503.387970	359577.784542	48.248551
3503.367566	359580.943119	48.253556
3503.413337	359583.989449	48.258561
3503.472471	359575.608225	48.263565
3503.643766	359569.244981	48.268570
3503.250941	359565.999042	48.273575
3503.297752	359559.909941	48.278580
3503.361183	359558.245891	48.283585
3503.622936	359551.512095	48.288589
3503.526516	359541.348759	48.293594
3503.605277	359555.509968	48.298599
3503.730846	359545.362432	48.303604
3503.599461	359554.162218	48.308609
3503.750783	359545.308379	48.313613
3503.620032	359556.296458	48.318618
3503.375001	359540.761971	48.323623
3503.643126	359543.900385	48.328628
3503.370735	359543.994335	48.333633
3503.501980	359515.168205	48.338637
3503.359209	359515.394343	48.343642
3503.326558	359506.874938	48.348647
3503.352011	359501.654385	48.353652
3503.425988	359514.874844	48.358657
3503.240489	359508.033622	48.363661
3503.349736	359524.505649	48.368666
3503.544162	359513.329362	48.373671
3503.813597	359511.963548	48.378676
3503.639997	359521.736979	48.383681
3503.874284	359511.266891	48.388685
3503.450939	359515.837835	48.393690
3503.630861	359515.300458	48.398695
3503.635328	359514.790819	48.403700
3503.580439	359501.541887	48.408705
3503.655741	359492.598270	48.413709
3503.396938	359500.451244	48.418714
3503.732656	359492.509763	48.423719
3503.692701	359481.828558	48.428724
3503.347202	359486.870681	48.433729
3503.809656	359492.879274	48.438733
3503.529218	359487.528953	48.443738
3503.569312	359489.100291	48.448743
3503.660569	359486.846571	48.453748
3503.517154	359468.522332	48.458753
3503.550055	359448.236279	48.463757
3503.252640	359460.421266	48.468762
3503.428034	359457.925225	48.473767
3503.677435	359440.302270	48.478772
3503.894938	359458.411227	48.483777
3503.726401	359446.656144	48.488781
3503.879760	359451.721193	48.493786
3503.951250	359440.996915	48.498791
3503.669745	359436.003007	48.503796
3503.371110	359436.177446	48.508801
3503.598572	359429.118249	48.513805
3503.685786	359432.361609	48.518810
3503.558897	359419.861987	48.523815
3503.864811	359419.915407	48.528820
3503.573866	359419.147110	48.533825
3503.779167	359416.061069	48.538829
3503.620562	359403.744582	48.543834
3503.414677	359393.776645	48.548839
3503.730803	359383.395378	48.553844
3503.607310	359393.466272	48.558849
3503.751332	359381.814440	48.563853
3503.393462	359394.263466	48.568858
3503.351631	359390.834795	48.573863
3503.550044	359388.106093	48.578868
3503.294267	359385.703658	48.583873
3503.756493	359383.238608	48.588877
3503.644031	359379.744762	48.593882
3503.587235	359360.567053	48.598887
3503.390709	359366.654392	48.603892
3503.612299	359354.634039	48.608897
3503.545236	359346.603530	48.613901
3503.453508	359346.338115	48.618906
3503.326265	359352.643522	48.623911
3503.650954	359345.034566	48.628916
3503.675584	359353.657045	48.633921
3503.703438	359344.797241	48.638925
3503.420088	359355.198773	48.643930
3503.635871	359353.866883	48.648935
3503.654136	359328.671912	48.653940
3503.387944	359329.451939	48.658945
3503.696426	359315.534795	48.663949
3503.436829	359322.700866	48.668954
3503.378548	359324.669460	48.673959
3503.293204	359324.810181	48.678964
3503.271608	359327.256460	48.683969
3503.285221	359326.745372	48.688973
3503.334822	359326.508507	48.693978
3503.287090	359320.052624	48.698983
3503.554795	359321.308073	48.703988
3503.311879	359328.395167	48.708993
3503.584911	359320.947052	48.713997
3503.674095	359328.134324	48.719002
3503.666026	359324.573078	48.724007
3503.764524	359326.465993	48.729012
3503.298902	359339.033854	48.734017
3503.474106	359319.819453	48.739021
3503.380186	359314.057928	48.744026
3503.262931	359298.299591	48.749031
3503.128632	359305.216837	48.754036
3503.149823	359318.420247	48.759041
3503.448958	359317.405984	48.764045
3503.471606	359326.512266	48.769050
3503.357565	359322.891433	48.774055
3503.363198	359309.276630	48.779060
3503.608467	359307.990970	48.784065
3503.577958	359300.005568	48.789069
3503.508053	359306.988973	48.794074
3503.620014	359294.782364	48.799079
3503.684256	359296.298998	48.804084
3503.383842	359309.247895	48.809089
3503.288284	359304.708062	48.814093
3503.256994	359301.684863	48.819098
3503.567314	359312.068892	48.824103
3503.420062	359313.415387	48.829108
3503.425864	359312.142138	48.834113
3503.616709	359304.503441	48.839117
3503.281698	359310.663573	48.844122
3503.378385	359309.630422	48.849127
3503.550181	359313.216670	48.854132
3503.372084	359321.616738	48.859137
3503.551626	359305.277106	48.864141
3503.358852	359284.263264	48.869146
3503.602915	359279.135361	48.874151
3503.385831	359277.948240	48.879156
3503.454360	359277.377577	48.884161
3503.447940	359270.686137	48.889165
3503.306359	359277.299180	48.894170
3503.161686	359275.998824	48.899175
3503.684416	359270.674187	48.904180
3503.097436	359283.821072	48.909185
3503.387138	359278.202469	48.914189
3503.510834	359279.709705	48.919194
3503.309952	359280.428515	48.924199
3503.174422	359277.243668	48.929204
3503.389122	359281.332068	48.934209
3503.162101	359276.304084	48.939213
3503.146561	359283.431578	48.944218
3503.276939	359285.523028	48.949223
3503.414783	359280.081112	48.954228
3503.309479	359290.937995	48.959233
3503.317855	359280.096426	48.964237
3503.562617	359290.287251	48.969242
3503.637727	359292.972709	48.974247
3503.464168	359288.826905	48.979252
3503.524621	359287.265103	48.984257
3503.503843	359284.062115	48.989261
3503.391990	359281.535136	48.994266
3503.528950	359291.921128	48.999271
3503.574666	359285.603147	49.004276
3503.275646	359293.920550	49.009281
3503.524880	359294.186503	49.014285
3503.349771	359290.498983	49.019290
3503.426322	359296.670393	49.024295
3503.473873	359291.980703	49.029300
3503.368240	359286.958977	49.034305
3503.455062	359273.789367	49.039309
3503.327259	359276.532351	49.044314
3503.295331	359269.437798	49.049319
3503.679434	359263.142658	49.054324
3503.362879	359264.643153	49.059329
3503.134493	359257.274297	49.064333
3503.280386	359269.872735	49.069338
3503.288775	359272.237937	49.074343
3503.351018	359274.263819	49.079348
3503.300032	359277.147339	49.084353
3503.560830	359261.151098	49.089357
3503.502735	359277.955022	49.094362
3503.191871	359268.945179	49.099367
3503.301410	359271.116264	49.104372
3503.244565	359269.649345	49.109377
3503.525873	359273.599982	49.114381
3503.384967	359276.039679	49.119386
3503.509750	359266.452033	49.124391
3503.775292	359267.835059	49.129396
3503.634016	359268.315427	49.134401
3503.712562	359274.613758	49.139405
3503.423600	359275.880871	49.144410
3503.560424	359276.393614	49.149415
3503.966201	359259.305697	49.154420
3503.367152	359246.015489	49.159425
3503.406258	359243.413750	49.164429
3503.449236	359241.243991	49.169434
3503.721261	359232.803605	49.174439
3503.560100	359237.587592	49.179444
3503.690743	359244.946448	49.184449
3503.970059	359238.057152	49.189453
3503.718508	359243.109895	49.194458
3503.505201	359216.042980	49.199463
3503.473860	359205.538479	49.204468
3503.613065	359198.035163	49.209473
3503.587210	359200.634801	49.214477
3503.615032	359206.941159	49.219482
3503.673864	359201.537172	49.224487
3503.589141	359200.736270	49.229492
3503.593051	359214.298693	49.234497
3503.362547	359200.059578	49.239501
3503.378249	359208.352688	49.244506
3503.482004	359199.760772	49.249511
3503.765134	359204.728991	49.254516
3503.403028	359180.764620	49.259521
3503.618562	359174.139865	49.264525
3503.439434	359167.094015	49.269530
3503.772456	359159.458266	49.274535
3503.685089	359171.482886	49.279540
3503.186978	359177.846945	49.284545
3503.551144	359165.854900	49.289549
3503.522223	359169.320210	49.294554
3503.187509	359168.100788	49.299559
3503.640190	359178.207873	49.304564
3503.467669	359175.639586	49.309569
3503.433184	359185.645559	49.314573
3503.158231	359175.764836	49.319578
3503.206484	359175.680864	49.324583
3503.314964	359169.378392	49.329588
3503.393238	359181.758523	49.334593
3503.419122	359176.512421	49.339597
3503.287082	359173.708715	49.344602
3503.168797	359188.486454	49.349607
3503.627275	359176.581288	49.354612
3503.145997	359180.118110	49.359617
3503.515762	359179.169018	49.364621
3503.312159	359186.529830	49.369626
3503.312068	359175.918596	49.374631
3503.674778	359180.619771	49.379636
3503.231402	359184.048814	49.384641
3503.421508	359180.049083	49.389645
3503.035121	359179.015957	49.394650
3502.898983	359187.460308	49.399655
3503.465861	359193.350643	49.404660
3503.388312	359191.759762	49.409665
3503.550140	359183.362234	49.414669
3503.361271	359196.115400	49.419674
3503.614128	359186.482045	49.424679
3503.612412	359177.703226	49.429684
3503.258719	359166.817084	49.434689
3503.560935	359152.315612	49.439693
3503.583213	359156.943374	49.444698
3503.226409	359158.959168	49.449703
3503.223732	359157.305555	49.454708
3503.301245	359161.390206	49.459713
3503.464694	359151.796425	49.464717
3503.334545	359159.985368	49.469722
3503.498331	359157.440254	49.474727
3503.629427	359154.035122	49.479732
3503.296596	359165.080682	49.484737
3503.414138	359153.865575	49.489741
3503.358542	359164.994541	49.494746
3503.595701	359155.210982	49.499751
3503.498078	359166.397485	49.504756
3503.508159	359161.790046	49.509761
3503.573550	359155.265364	49.514765
3503.400951	359169.822676	49.519770
3503.561856	359165.344073	49.524775
3503.548171	359160.842178	49.529780
3503.427595	359154.525022	49.534785
3503.632642	359131.666959	49.539789
3503.672181	359134.078136	49.544794
3503.555364	359125.215716	49.549799
3503.726488	359132.339169	49.554804
3503.210061	359131.810087	49.559809
3503.554422	359127.149798	49.564813
3503.193419	359133.008702	49.569818
3503.320735	359130.291225	49.574823
3503.492186	359128.101151	49.579828
3503.488014	359133.750963	49.584833
3503.421342	359129.537354	49.589837
3503.448593	359136.708998	49.594842
3503.277143	359138.186557	49.599847
3503.648856	359136.804564	49.604852
3503.523090	359133.312804	49.609857
3503.687091	359133.592233	49.614861
3503.656298	359102.730296	49.619866
3503.359815	359104.685663	49.624871
3503.804888	359095.454496	49.629876
3503.498636	359098.352934	49.634881
3503.510822	359097.485817	49.639885
3503.523499	359095.244501	49.644890
3503.572696	359090.579978	49.649895
3503.752341	359096.760562	49.654900
3503.573827	359095.083852	49.659905
3503.662546	359073.999973	49.664909
3503.540795	359071.983481	49.669914
3503.259085	359060.373429	49.674919
3503.573670	359059.254931	49.679924
3503.496067	359065.934228	49.684929
3503.644586	359053.136505	49.689933
3503.723653	359061.165156	49.694938
3503.600671	359059.123412	49.699943
3503.570084	359065.744383	49.704948
3503.352528	359057.712171	49.709953
3503.842838	359061.197191	49.714957
3503.898275	359045.818619	49.719962
3503.430443	359040.319746	49.724967
3503.674375	359024.682349	49.729972
3503.430855	359035.204886	49.734977
3503.363775	359029.718997	49.739981
3503.375756	359039.870334	49.744986
3503.334937	359031.759284	49.749991
3503.388608	359039.842847	49.754996
3503.294587	359034.233985	49.760001
3503.750655	359027.240378	49.765005
3503.504362	359031.885163	49.770010
3503.191950	359035.929681	49.775015
3503.524899	359026.512653	49.780020
3503.494745	359043.185007	49.785025
3503.610608	359029.476360	49.790029
3503.311218	359028.276797	49.795034
3503.428987	359020.496928	49.800039
3503.329006	359005.651848	49.805044
3503.245582	359002.255172	49.810049
3503.330691	359001.758225	49.815053
3503.079986	359022.536928	49.820058
3503.245654	359027.218375	49.825063
3503.368188	359036.156240	49.830068
3503.259234	359045.614186	49.835073
3503.492475	359042.396472	49.840077
3503.648979	359034.508695	49.845082
3503.487606	359020.716639	49.850087
3503.582214	359007.087686	49.855092
3503.097992	359005.637428	49.860097
3503.303199	359001.431721	49.865101
3503.223261	359004.090813	49.870106
3503.219690	359006.941406	49.875111
3503.618479	359007.998013	49.880116
3503.301064	359016.471052	49.885121
3503.475841	359011.761222	49.890125
3503.612948	359017.515947	49.895130
3503.486232	359014.202455	49.900135
3503.452175	359014.742216	49.905140
3503.327459	359015.957923	49.910145
3503.356583	359016.513143	49.915149
3503.431104	359012.531670	49.920154
3503.678397	359011.958191	49.925159
3503.849769	359009.259189	49.930164
3503.437131	359024.694233	49.935169
3503.823357	359006.362430	49.940173
3503.463080	359002.933181	49.945178
3503.637175	358987.917533	49.950183
3503.332606	358980.077191	49.955188
3503.382145	358994.421311	49.960193
3503.564599	358990.677240	49.965197
3503.612403	358995.682684	49.970202
3503.638310	358999.851847	49.975207
3503.802566	358986.517238	49.980212
3503.567881	358996.249538	49.985217
3503.482407	358990.919233	49.990221
3503.303363	358986.265336	49.995226
3503.360133	358990.913108	50.000231
3503.669641	358985.520361	50.005236
3503.161042	358975.651088	50.010241
3503.507719	358949.844176	50.015245
3503.343695	358960.226927	50.020250
3503.376018	358957.193651	50.025255
3503.666844	358942.312216	50.030260
3503.596032	358955.708396	50.035265
3503.442426	358954.714805	50.040269
3503.666080	358957.834840	50.045274
3503.502739	358960.252652	50.050279
3503.749012	358958.076189	50.055284
3503.369770	358973.302395	50.060289
3503.709107	358948.539959	50.065293
3503.597869	358963.978267	50.070298
3503.457926	358933.464287	50.075303
3503.309734	358928.678273	50.080308
3503.411729	358919.603098	50.085313
3503.610368	358912.751957	50.090317
3503.284265	358922.422384	50.095322
3503.429955	358917.691696	50.100327
3503.908836	358908.887745	50.105332
3503.480945	358927.277056	50.110337
3503.574643	358928.254663	50.115341
3503.607179	358920.488253	50.120346
3503.430505	358922.322899	50.125351
3503.700934	358916.300153	50.130356
3503.635280	358931.960287	50.135361
3503.521433	358893.400980	50.140365
3503.554450	358896.245796	50.145370
3503.600144	358888.070152	50.150375
3503.985893	358876.761687	50.155380
3503.418630	358893.417215	50.160385
3503.624652	358879.159890	50.165389
3503.678835	358882.688423	50.170394
3503.721985	358877.108752	50.175399
3503.605206	358867.559217	50.180404
3503.424842	358853.566542	50.185409
3503.522621	358843.321466	50.190413
3503.700430	358840.316076	50.195418
3503.815153	358851.011039	50.200423
3503.782578	358843.636612	50.205428
3503.169232	358847.601485	50.210433
3503.077677	358848.964635	50.215437
3503.333197	358851.672490	50.220442
3503.419612	358849.826655	50.225447
3503.387281	358850.900527	50.230452
3503.192772	358858.972461	50.235457
3503.687854	358849.555215	50.240461
3503.665318	358858.465153	50.245466
3503.535865	358859.299911	50.250471
3503.689629	358837.925732	50.255476
3502.987370	358817.246702	50.260481
3503.178858	358833.197024	50.265485
3503.732859	358829.623226	50.270490
3503.581470	358825.270303	50.275495
3503.746818	358812.800665	50.280500
3503.247368	358820.564557	50.285505
3503.451118	358805.340591	50.290509
3503.629154	358810.808955	50.295514
3503.240740	358822.295976	50.300519
3503.526607	358813.039032	50.305524
3503.530360	358814.870605	50.310529
3503.778367	358814.475138	50.315533
3503.732371	358824.915600	50.320538
3503.609561	358821.983180	50.325543
3503.891942	358799.112737	50.330548
3503.431115	358793.078345	50.335553
3503.567232	358779.544553	50.340557
3503.607262	358780.581541	50.345562
3503.450037	358783.812694	50.350567
3503.730638	358783.793777	50.355572
3503.600219	358789.870736	50.360577
3503.435644	358787.861003	50.365581
3503.416764	358784.301427	50.370586
3503.353314	358785.914604	50.375591
3503.556023	358787.383917	50.380596
3503.200841	358790.722704	50.385601
3503.307317	358783.046370	50.390605
3503.365423	358786.930546	50.395610
3503.205321	358787.592023	50.400615
3503.558782	358787.408906	50.405620
3502.958633	358795.315956	50.410625
3503.323427	358778.590606	50.415629
3503.514500	358792.021770	50.420634
3503.397154	358787.739803	50.425639
3503.187155	358784.006865	50.430644
3503.201454	358798.203932	50.435649
3503.400270	358794.864410	50.440653
3503.264794	358796.005483	50.445658
3503.141276	358799.816583	50.450663
3503.303718	358794.268937	50.455668
3503.465820	358797.424160	50.460673
3503.374718	358790.542467	50.465677
3503.386707	358796.902275	50.470682
3503.522868	358799.679896	50.475687
3503.549995	358784.992782	50.480692
3503.210725	358773.671676	50.485697
3503.264793	358759.107530	50.490701
3503.553747	358758.400227	50.495706
3503.428519	358766.690245	50.500711
3503.470186	358758.947813	50.505716
3503.158820	358765.816787	50.510721
3503.519097	358760.975820	50.515725
3503.569765	358765.421003	50.520730
3503.389860	358757.662705	50.525735
3503.651274	358731.283879	50.530740
3502.893900	358713.489013	50.535745
3502.946021	358668.490680	50.540749
3502.811714	358623.140074	50.545754
3502.766633	358572.355122	50.550759
3502.581400	358504.644589	50.555764
3502.514536	358448.442746	50.560769
3502.300559	358366.333558	50.565773
3501.607787	358279.643107	50.570778
3501.987896	358183.647369	50.575783
3501.750003	358079.198885	50.580788
3501.038491	357974.926845	50.585793
3501.164916	357858.918143	50.590797
3500.539721	357744.173125	50.595802
3499.858201	357629.742115	50.600807
3499.906135	357497.865781	50.605812
3499.190623	357363.768615	50.610817
3498.910649	357228.609776	50.615821
3498.435973	357090.529419	50.620826
3498.023171	356946.255090	50.625831
3497.704964	356806.673244	50.630836
3496.821097	356651.173692	50.635841
3496.623852	356497.753639	50.640845
3496.301871	356351.300165	50.645850
3495.435011	356180.756658	50.650855
3495.189351	356008.740164	50.655860
3494.534683	355852.413025	50.660865
3494.206189	355683.716808	50.665869
3493.692029	355517.314302	50.670874
3492.826539	355341.576270	50.675879
3492.536187	355162.336587	50.680884
3491.439145	354986.633944	50.685889
3491.263030	354803.735776	50.690893
3490.492859	354625.944317	50.695898
3489.692143	354448.462463	50.700903
3488.980936	354265.112553	50.705908
3488.474070	354091.476734	50.710913
3488.067907	353915.788472	50.715917
3487.642810	353727.225228	50.720922
3487.124921	353546.997949	50.725927
3486.451404	353355.062408	50.730932
3485.769938	353168.879043	50.735937
3484.979574	352980.803505	50.740941
3484.410507	352782.410578	50.745946
3483.635589	352591.099081	50.750951
3482.762205	352409.804317	50.755956
3482.257084	352224.124195	50.760961
3481.970884	352034.234984	50.765965
3481.589882	351845.658051	50.770970
3480.608894	351652.975997	50.775975
3480.405223	351458.337926	50.780980
3479.212699	351262.481157	50.785985
3478.598476	351058.871602	50.790989
3478.024541	350853.422456	50.795994
3477.260308	350665.512798	50.800999
3476.900063	350466.925583	50.806004
3475.919272	350263.930921	50.811009
3475.522332	350061.123161	50.816013
3474.950391	349875.980008	50.821018
3474.348097	349668.189374	50.826023
3473.969101	349468.430746	50.831028
3473.255983	349272.389236	50.836033
3472.650534	349068.134601	50.841037
3471.992742	348857.550024	50.846042
3471.295098	348642.491440	50.851047
3470.435827	348438.071011	50.856052
3469.803090	348244.329294	50.861057
3469.362717	348027.395133	50.866061
3468.657886	347818.213950	50.871066
3467.859668	347626.481540	50.876071
3467.108852	347408.906878	50.881076
3466.351235	347206.680269	50.886081
3465.669900	346997.823230	50.891085
3465.098196	346796.660233	50.896090
3464.403098	346588.516549	50.901095
3463.786925	346387.995469	50.906100
3462.885571	346183.828114	50.911105
3462.466571	345975.485848	50.916109
3461.956557	345773.444128	50.921114
3460.679172	345579.260788	50.926119
3460.414422	345362.645122	50.931124
3459.727315	345177.072123	50.936129
3458.965180	344960.991771	50.941133
3458.300958	344765.945187	50.946138
3457.341144	344557.861555	50.951143
3456.939364	344346.761789	50.956148
3455.935782	344159.046611	50.961153
3455.461501	343956.433022	50.966157
3454.774875	343754.437759	50.971162
3453.824359	343557.497978	50.976167
3453.569370	343353.829518	50.981172
3453.166190	343155.580087	50.986177
3452.565059	342949.368664	50.991181
3451.821122	342749.237255	50.996186
3450.621115	342529.908288	51.001191
3450.349025	342334.537255	51.006196
3449.620496	342127.452285	51.011201
3449.048271	341936.658358	51.016205
3448.304365	341726.443541	51.021210
3447.471613	341535.002285	51.026215
3446.849764	341318.046700	51.031220
3446.085252	341120.815103	51.036225
3445.496221	340925.922462	51.041229
3444.709181	340714.361920	51.046234
3444.239659	340519.729125	51.051239
3443.505905	340310.551592	51.056244
3442.622272	340115.041176	51.061249
3441.990900	339909.409887	51.066253
3441.274608	339717.868302	51.071258
3440.718529	339521.566055	51.076263
3440.185525	339306.676859	51.081268
3439.241190	339110.001991	51.086273
3438.778434	338907.675531	51.091277
3437.943401	338713.502304	51.096282
3437.297187	338512.145485	51.101287
3436.806081	338315.014693	51.106292
3435.957962	338123.692858	51.111297
3435.182318	337918.892624	51.116301
3434.645510	337719.883496	51.121306
3433.619017	337527.518957	51.126311
3433.187963	337326.302663	51.131316
3432.593390	337134.250532	51.136321
3431.901172	336939.693075	51.141325
3431.333002	336749.824932	51.146330
3430.382533	336541.153193	51.151335
3430.100510	336341.412311	51.156340
3429.193433	336151.366949	51.161345
3428.570553	335953.766285	51.166349
3428.049813	335746.831587	51.171354
3426.781272	335565.624442	51.176359
3426.360338	335355.414250	51.181364
3425.734713	335167.663700	51.186369
3425.145632	334957.911650	51.191373
3424.159051	334779.483613	51.196378
3423.552483	334576.097537	51.201383
3423.507771	334374.378599	51.206388
3422.521318	334192.003095	51.211393
3421.855250	333996.949399	51.216397
3421.458734	333794.469763	51.221402
3420.346694	333604.118820	51.226407
3419.948100	333400.390939	51.231412
3419.326879	333202.247531	51.236417
3418.422010	332993.252340	51.241421
3417.701129	332804.492174	51.246426
3416.863637	332615.546282	51.251431
3416.281266	332413.957673	51.256436
3415.620415	332231.831132	51.261441
3414.998319	332027.498215	51.266445
3414.306869	331826.281631	51.271450
3413.554074	331646.892221	51.276455
3412.628258	331450.192372	51.281460
3412.191463	331266.627754	51.286465
3411.445391	331078.961797	51.291469
3411.024091	330895.215590	51.296474
3410.136753	330696.267258	51.301479
3409.771941	330506.248254	51.306484
3408.893946	330319.594133	51.311489
3408.507865	330116.491536	51.316493
3408.137809	329924.358773	51.321498
3407.079449	329727.140668	51.326503
3406.225200	329527.827565	51.331508
3405.751489	329344.849618	51.336513
3405.334475	329140.170803	51.341517
3404.295635	328947.402991	51.346522
3403.561542	328761.180539	51.351527
3403.057300	328567.207014	51.356532
3402.342073	328376.958023	51.361537
3401.615506	328183.757023	51.366541
3401.245088	327988.436977	51.371546
3400.100959	327796.650418	51.376551
3399.645015	327606.307623	51.381556
3398.810243	327412.816308	51.386561
3398.281336	327218.486888	51.391565
3397.767193	327030.112333	51.396570
3396.882324	326838.282445	51.401575
3396.408221	326633.937062	51.406580
3395.808421	326455.784268	51.411585
3395.188235	326257.546048	51.416589
3394.542639	326062.570299	51.421594
3393.818005	325878.478221	51.426599
3393.114509	325676.840044	51.431604
3392.324178	325484.686460	51.436609
3391.929084	325281.496360	51.441613
3391.196131	325092.413529	51.446618
3390.276592	324900.329934	51.451623
3389.982802	324692.182963	51.456628
3388.925179	324506.689202	51.461633
3388.530496	324317.372888	51.466637
3388.029098	324116.055400	51.471642
3387.108511	323925.599237	51.476647
3386.632179	323732.882730	51.481652
3385.826912	323538.257287	51.486657
3385.163599	323334.341040	51.491661
3384.330199	323139.566370	51.496666
3383.460019	322955.847328	51.501671
3383.072027	322761.459672	51.506676
3382.272963	322567.543971	51.511681
3381.451478	322388.730100	51.516685
3380.908773	322192.787021	51.521690
3380.202729	321999.542813	51.526695
3379.772169	321807.374933	51.531700
3378.955623	321621.734972	51.536705
3378.132645	321428.227928	51.541709
3377.958777	321237.291313	51.546714
3376.947335	321050.586122	51.551719
3376.384815	320850.722074	51.556724
3375.627215	320670.825236	51.561729
3374.910096	320474.905965	51.566733
3374.149134	320286.275388	51.571738
3373.642850	320097.502298	51.576743
3373.377631	319907.188423	51.581748
3372.268832	319715.148811	51.586753
3371.695027	319521.725614	51.591757
3371.287209	319332.909928	51.596762
3370.137915	319151.289693	51.601767
3369.656864	318952.630839	51.606772
3368.837124	318758.099144	51.611777
3367.989457	318573.170882	51.616781
3367.537451	318384.003807	51.621786
3366.767734	318189.208410	51.626791
3366.333919	318000.801584	51.631796
3365.380190	317823.705726	51.636801
3365.102601	317633.923946	51.641805
3364.632868	317433.885155	51.646810
3363.650281	317250.197913	51.651815
3363.076801	317055.725689	51.656820
3362.595822	316867.706077	51.661825
3361.681181	316671.071760	51.666829
3360.847452	316478.320126	51.671834
3360.056937	316309.445803	51.676839
3359.688235	316113.029608	51.681844
3358.811261	315938.006220	51.686849
3357.749452	315741.673454	51.691853
3357.384248	315558.216488	51.696858
3356.516392	315370.662679	51.701863
3355.906968	315181.005111	51.706868
3355.446083	315009.148196	51.711873
3354.801390	314820.717797	51.716877
3354.111682	314636.954024	51.721882
3353.521775	314453.607028	51.726887
3353.021695	314254.330669	51.731892
3352.059681	314072.340510	51.736897
3351.360753	313882.440109	51.741901
3350.737200	313706.685363	51.746906
3350.008758	313517.476506	51.751911
3349.833486	313322.475904	51.756916
3348.906214	313151.428192	51.761921
3348.134343	312965.128136	51.766925
3347.442881	312779.680824	51.771930
3346.532891	312599.462443	51.776935
3346.161749	312408.081632	51.781940
3345.685615	312221.020549	51.786945
3344.789698	312031.453652	51.791949
3344.264235	311855.604034	51.796954
3343.649440	311663.496555	51.801959
3343.196771	311478.645925	51.806964
3342.222895	311280.152099	51.811969
3341.588094	311090.695119	51.816973
3341.206053	310910.823438	51.821978
3340.045319	310725.599755	51.826983
3339.879141	310530.694722	51.831988
3338.721790	310337.219358	51.836993
3337.918699	310161.843962	51.841997
3337.579434	309974.426533	51.847002
3336.805316	309792.909012	51.852007
3336.410764	309605.601606	51.857012
3335.650799	309422.782583	51.862017
3334.547573	309226.623050	51.867021
3334.120863	309045.278642	51.872026
3333.412923	308857.255698	51.877031
3332.867088	308673.357621	51.882036
3332.011948	308492.614923	51.887041
3331.141169	308297.206559	51.892045
3330.621384	308128.582594	51.897050
3329.942097	307949.390134	51.902055
3329.259881	307765.206709	51.907060
3328.568030	307588.078405	51.912065
3327.937985	307408.520881	51.917069
3327.756994	307226.039972	51.922074
3326.740512	307050.159138	51.927079
3326.490955	306850.168408	51.932084
3325.361432	306677.004277	51.937089
3324.773761	306490.512199	51.942093
3323.824922	306305.273858	51.947098
3323.498788	306121.311907	51.952103
3323.236299	305928.350305	51.957108
3322.032802	305751.580566	51.962113
3321.743226	305565.702157	51.967117
3321.004610	305386.541047	51.972122
3319.898446	305200.078259	51.977127
3319.774890	305014.885885	51.982132
3318.851921	304837.688615	51.987137
3318.294527	304651.291089	51.992141
3317.717859	304458.249791	51.997146
3316.862528	304274.827459	52.002151
3316.012078	304090.309087	52.007156
3315.520631	303930.435615	52.012161
3314.543992	303728.314338	52.017165
3313.972291	303552.307742	52.022170
3313.098486	303375.533806	52.027175
3312.958419	303192.735486	52.032180
3312.287394	303016.285571	52.037185
3311.506918	302828.316623	52.042189
3310.866494	302645.138383	52.047194
3310.023247	302458.579539	52.052199
3309.381808	302285.129094	52.057204
3308.704380	302106.463572	52.062209
3308.397755	301925.727362	52.067213
3307.453579	301741.806634	52.072218
3306.253558	301572.594743	52.077223
3306.228412	301375.438547	52.082228
3305.205554	301196.928490	52.087233
3304.400532	301034.274800	52.092237
3304.071191	300847.097954	52.097242
3303.350990	300682.978909	52.102247
3302.912795	300485.275760	52.107252
3302.177641	300321.184183	52.112257
3301.539496	300123.945158	52.117261
3301.100184	299944.297302	52.122266
3300.116837	299760.074923	52.127271
3299.768493	299575.930169	52.132276
3299.006713	299401.273265	52.137281
3298.150370	299215.196611	52.142285
3297.529551	299034.506908	52.147290
3296.560837	298851.427241	52.152295
3296.104281	298677.816400	52.157300
3295.239726	298499.813241	52.162305
3294.551440	298313.836386	52.167309
3294.075091	298139.413215	52.172314
3293.233280	297967.849036	52.177319
3292.724286	297792.590291	52.182324
3291.900923	297613.841208	52.187329
3291.493678	297426.545653	52.192333
3290.347464	297251.514526	52.197338
3289.929721	297082.021674	52.202343
3289.406086	296889.981676	52.207348
3288.618513	296721.183678	52.212353
3287.925999	296547.964701	52.217357
3287.661992	296361.867863	52.222362
3286.348876	296185.104943	52.227367
3285.846197	296017.305426	52.232372
3285.432962	295842.895636	52.237377
3284.810801	295656.803859	52.242381
3284.186964	295483.318423	52.247386
3283.556687	295312.049505	52.252391
3282.775201	295124.658155	52.257396
3282.097494	294944.151841	52.262401
3281.290561	294767.664173	52.267405
3281.010683	294602.502325	52.272410
3279.685827	294412.827843	52.277415
3279.384380	294234.451602	52.282420
3279.001772	294057.692495	52.287425
3278.170053	293886.097760	52.292429
3277.711029	293711.948138	52.297434
3276.825377	293522.738234	52.302439
3276.339547	293342.684133	52.307444
3275.343614	293160.876926	52.312449
3274.669363	292989.664088	52.317453
3274.015239	292808.082681	52.322458
3273.285393	292633.720413	52.327463
3272.862320	292461.092218	52.332468
3271.835420	292289.781857	52.337473
3270.844648	292110.901801	52.342477
3270.460826	291938.547172	52.347482
3269.821541	291770.358583	52.352487
3269.486897	291589.515231	52.357492
3268.752958	291423.913613	52.362497
3268.029427	291236.891965	52.367501
3267.676924	291058.597831	52.372506
3266.900528	290883.783299	52.377511
3266.557036	290706.302469	52.382516
3265.520498	290527.046544	52.387521
3264.693639	290352.010442	52.392525
3264.333263	290171.832359	52.397530
3263.544765	290005.958356	52.402535
3263.095688	289807.406357	52.407540
3262.121782	289637.664902	52.412545
3261.135619	289455.700745	52.417549
3260.753395	289283.496982	52.422554
3260.141101	289112.220889	52.427559
3259.644377	288932.445627	52.432564
3258.945793	288754.866959	52.437569
3258.276697	288582.911924	52.442573
3257.764817	288398.452662	52.447578
3256.774792	288222.396936	52.452583
3256.153917	288035.866341	52.457588
3255.460936	287859.890769	52.462593
3254.740981	287682.671443	52.467597
3254.478206	287508.690535	52.472602
3253.630923	287334.547324	52.477607
3252.677432	287166.685950	52.482612
3252.183997	286988.895608	52.487617
3251.665492	286806.346626	52.492621
3251.071593	286624.879138	52.497626
3250.030638	286458.814034	52.502631
3249.470127	286275.176312	52.507636
3248.613541	286116.442156	52.512641
3248.095331	285940.387062	52.517645
3247.556891	285758.528369	52.522650
3246.936119	285581.979981	52.527655
3246.363177	285412.172994	52.532660
3245.556862	285228.853826	52.537665
3244.927476	285047.773252	52.542669
3244.122418	284871.992295	52.547674
3243.332808	284695.444780	52.552679
3242.852444	284516.148651	52.557684
3241.981308	284346.846852	52.562689
3241.242626	284172.990705	52.567693
3240.884761	283992.910952	52.572698
3239.764576	283827.595935	52.577703
3239.472230	283652.599330	52.582708
3238.700012	283489.979720	52.587713
3237.830553	283310.642829	52.592717
3237.221704	283143.769545	52.597722
3236.154251	282975.924563	52.602727
3235.825948	282799.481676	52.607732
3234.976674	282637.994604	52.612737
3234.559368	282458.127481	52.617741
3234.041551	282291.010331	52.622746
3233.323756	282132.100085	52.627751
3232.835074	281954.790931	52.632756
3231.819487	281783.219043	52.637761
3231.312099	281611.006411	52.642765
3230.745855	281451.919214	52.647770
3229.995342	281282.903031	52.652775
3229.613647	281103.793950	52.657780
3228.711563	280932.509518	52.662785
3227.781658	280765.049697	52.667789
3227.719617	280590.627032	52.672794
3226.617689	280424.238556	52.677799
3226.046518	280242.485084	52.682804
3225.369267	280081.301299	52.687809
3224.830474	279902.038533	52.692813
3224.421501	279736.635440	52.697818
3223.318275	279568.489699	52.702823
3223.029640	279384.806708	52.707828
3222.108682	279212.659013	52.712833
3221.234629	279048.017036	52.717837
3220.602554	278868.081208	52.722842
3219.897446	278704.533065	52.727847
3219.361235	278537.112459	52.732852
3218.497957	278376.288948	52.737857
3218.054913	278208.497007	52.742861
3217.398852	278027.851751	52.747866
3216.087533	277862.743980	52.752871
3215.746986	277694.273594	52.757876
3214.774983	277542.992380	52.762881
3214.530212	277378.989251	52.767885
3213.976835	277213.736047	52.772890
3213.326280	277051.809097	52.777895
3212.683602	276875.440316	52.782900
3212.146538	276716.908157	52.787905
3211.528684	276545.043337	52.792909
3211.091031	276363.472012	52.797914
3209.668993	276200.317258	52.802919
3208.989108	276021.280150	52.807924
3208.645787	275867.734588	52.812929
3207.829680	275704.687709	52.817933
3207.034554	275537.511630	52.822938
3206.193072	275376.480769	52.827943
3205.746371	275213.681069	52.832948
3205.008985	275050.163309	52.837953
3204.194271	274886.301230	52.842957
3204.132955	274722.141680	52.847962
3203.368670	274566.090429	52.852967
3202.856312	274393.444874	52.857972
3202.233131	274227.846137	52.862977
3201.326039	274056.307257	52.867981
3200.976508	273885.189542	52.872986
3199.749588	273721.927575	52.877991
3199.480562	273539.438251	52.882996
3198.577622	273391.176865	52.888001
3197.910485	273217.435276	52.893005
3197.575332	273050.313894	52.898010
3196.468386	272894.469785	52.903015
3196.066331	272728.810720	52.908020
3194.977367	272561.452101	52.913025
3194.371800	272391.852211	52.918029
3194.041368	272227.022332	52.923034
3193.253112	272072.834278	52.928039
3192.725222	271906.201964	52.933044
3192.103191	271738.947862	52.938049
3191.563331	271579.779718	52.943053
3190.985824	271406.024198	52.948058
3190.197968	271238.694542	52.953063
3189.637143	271064.809103	52.958068
3189.030688	270905.396926	52.963073
3188.428029	270727.672456	52.968077
3188.261095	270557.061148	52.973082
3186.871458	270390.463579	52.978087
3186.683037	270203.403220	52.983092
3185.603548	270041.926720	52.988097
3184.811677	269871.312570	52.993101
3184.470236	269698.080365	52.998106
3183.186819	269528.944827	53.003111
3182.953752	269358.649881	53.008116
3182.107569	269188.044496	53.013121
3181.338314	269019.642724	53.018125
3180.961427	268862.435883	53.023130
3179.783157	268694.888432	53.028135
3179.117502	268527.871159	53.033140
3178.362708	268362.090513	53.038145
3177.662495	268204.094557	53.043149
3177.393447	268044.986228	53.048154
3176.594830	267889.705563	53.053159
3175.872591	267717.349166	53.058164
3175.275935	267561.425407	53.063169
3174.546414	267401.371405	53.068173
3174.037699	267241.639072	53.073178
3173.154775	267074.656638	53.078183
3172.554081	266909.794399	53.083188
3171.909898	266750.516624	53.088193
3171.262509	266596.103826	53.093197
3170.670388	266428.948270	53.098202
3169.772404	266272.257635	53.103207
3169.549913	266118.032454	53.108212
3168.552587	265952.927708	53.113217
3167.824723	265782.890518	53.118221
3167.199637	265624.246835	53.123226
3166.366229	265466.502091	53.128231
3165.965883	265300.946595	53.133236
3165.440431	265144.019165	53.138241
3164.439385	264981.462210	53.143245
3163.922827	264817.351518	53.148250
3162.983114	264669.938470	53.153255
3162.320662	264510.155093	53.158260
3161.975404	264347.851200	53.163265
3161.305343	264182.644487	53.168269
3160.618011	264016.600141	53.173274
3159.704520	263864.675441	53.178279
3159.388510	263698.903574	53.183284
3158.794878	263542.929936	53.188289
3158.162031	263386.071198	53.193293
3157.342490	263222.493078	53.198298
3156.795366	263065.799203	53.203303
3156.206242	262902.388527	53.208308
3155.388989	262740.389296	53.213313
3154.832483	262580.335383	53.218317
3154.029002	262413.189634	53.223322
3152.925060	262259.691343	53.228327
3152.378344	262094.873647	53.233332
3151.976130	261944.167811	53.238337
3151.000400	261786.141671	53.243341
3150.697287	261629.766462	53.248346
3149.841401	261472.969450	53.253351
3149.439241	261311.516531	53.258356
3148.921213	261158.537328	53.263361
3148.052582	260989.034196	53.268365
3147.331197	260826.969907	53.273370
3146.493863	260671.622065	53.278375
3146.292200	260499.747070	53.283380
3145.519716	260335.348132	53.288385
3144.787158	260180.187734	53.293389
3144.278951	260016.129190	53.298394
3143.241631	259874.260369	53.303399
3142.668850	259703.157709	53.308404
3142.111999	259550.007293	53.313409
3141.422837	259395.706397	53.318413
3141.137118	259224.329428	53.323418
3139.977572	259069.211802	53.328423
3139.120010	258904.394297	53.333428
3138.628923	258742.702351	53.338433
3137.839134	258585.132578	53.343437
3137.185036	258427.363165	53.348442
3136.464806	258266.166214	53.353447
3136.002224	258107.780957	53.358452
3135.308774	257960.663473	53.363457
3134.725589	257800.361986	53.368461
3133.953709	257638.307754	53.373466
3132.975533	257488.612489	53.378471
3132.663187	257326.842305	53.383476
3132.086228	257174.715297	53.388481
3131.314689	257026.617552	53.393485
3130.368352	256853.207607	53.398490
3129.743993	256710.740527	53.403495
3129.557043	256557.457138	53.408500
3128.746659	256402.922751	53.413505
3127.792908	256239.523101	53.418509
3127.388407	256082.377997	53.423514
3126.561276	255929.374639	53.428519
3125.869899	255779.202235	53.433524
3125.239180	255620.030438	53.438529
3124.652691	255466.072528	53.443533
3124.137860	255309.684020	53.448538
3123.375388	255154.837380	53.453543
3122.718841	255000.279703	53.458548
3121.897547	254845.391678	53.463553
3121.419763	254684.388264	53.468557
3120.876597	254525.738294	53.473562
3119.911356	254372.936252	53.478567
3119.558629	254210.869295	53.483572
3119.045585	254061.230248	53.488577
3118.602522	253895.994487	53.493581
3117.528961	253732.131992	53.498586
3116.560812	253583.151084	53.503591
3116.576567	253430.500167	53.508596
3115.394795	253272.996451	53.513601
3114.335353	253122.324087	53.518605
3114.222037	252950.466551	53.523610
3113.400030	252798.636343	53.528615
3112.691642	252642.331603	53.533620
3112.127339	252488.143405	53.538625
3111.295947	252330.457736	53.543629
3110.793769	252176.973046	53.548634
3110.094702	252020.387251	53.553639
3109.492924	251857.063010	53.558644
3108.752878	251709.830237	53.563649
3107.973651	251557.917939	53.568653
3107.467945	251390.962684	53.573658
3106.662198	251246.592967	53.578663
3106.119339	251085.704932	53.583668
3105.585397	250936.428364	53.588673
3104.810070	250773.616502	53.593677
3104.234921	250603.897181	53.598682
3103.175094	250460.867149	53.603687
3102.914811	250299.476770	53.608692
3102.101187	250155.160192	53.613697
3101.384056	250005.302275	53.618701
3100.677879	249840.112039	53.623706
3100.126909	249686.535511	53.628711
3099.346240	249529.990463	53.633716
3098.467464	249378.936342	53.638721
3097.961663	249229.147586	53.643725
3097.263574	249075.594941	53.648730
3096.234246	248936.050335	53.653735
3095.855829	248776.615646	53.658740
3095.401526	248629.187678	53.663745
3094.441493	248471.322390	53.668749
3094.016098	248334.102040	53.673754
3093.217132	248181.483046	53.678759
3092.650646	248024.472726	53.683764
3091.891898	247879.996803	53.688769
3091.128750	247727.754598	53.693773
3090.706282	247565.399589	53.698778
3089.481817	247425.250633	53.703783
3089.017827	247283.122449	53.708788
3088.576716	247144.632405	53.713793
3087.666983	246992.261377	53.718797
3087.248313	246849.286079	53.723802
3086.551853	246705.921970	53.728807
3086.110269	246551.210871	53.733812
3085.370134	246406.224171	53.738817
3084.998337	246244.983138	53.743821
3084.466600	246095.660075	53.748826
3083.418686	245941.122010	53.753831
3082.992972	245778.081994	53.758836
3082.071855	245631.724140	53.763841
3081.507038	245474.156138	53.768845
3080.903680	245313.462159	53.773850
3080.104925	245161.915945	53.778855
3079.653559	245015.790001	53.783860
3078.561828	244861.158244	53.788865
3077.695251	244708.808385	53.793869
3077.618318	244557.887118	53.798874
3076.706618	244423.064920	53.803879
3076.161466	244265.877217	53.808884
3075.478171	244120.247349	53.813889
3074.408146	243972.336045	53.818893
3074.028600	243817.872926	53.823898
3073.455701	243667.591423	53.828903
3072.740011	243517.078044	53.833908
3071.789358	243379.181816	53.838913
3071.353930	243230.305122	53.843917
3070.939441	243062.886701	53.848922
3069.850958	242922.288024	53.853927
3069.517160	242769.474172	53.858932
3068.850646	242623.588717	53.863937
3068.086104	242464.273444	53.868941
3067.522191	242318.626761	53.873946
3066.958573	242171.910677	53.878951
3066.278143	242021.393527	53.883956
3065.471009	241883.323461	53.888961
3064.672330	241731.195636	53.893965
3064.371386	241570.687708	53.898970
3063.381522	241412.580857	53.903975
3062.881970	241263.614841	53.908980
3062.157927	241116.441605	53.913985
3061.223321	240965.660434	53.918989
3061.039420	240822.425491	53.923994
3060.129562	240664.918129	53.928999
3059.762734	240506.331915	53.934004
3058.775919	240363.122756	53.939009
3058.284992	240217.441627	53.944013
3057.590913	240062.574703	53.949018
3056.898457	239920.949230	53.954023
3056.580677	239760.879342	53.959028
3055.468705	239609.618723	53.964033
3054.566643	239464.843950	53.969037
3054.398255	239317.585061	53.974042
3053.222855	239167.048075	53.979047
3052.694712	238999.958963	53.984052
3052.139026	238868.957206	53.989057
3051.233120	238725.024317	53.994061
3050.957922	238569.507471	53.999066
3049.830229	238430.219075	54.004071
3049.301609	238275.175647	54.009076
3048.884850	238127.652081	54.014081
3048.096309	237975.400331	54.019085
3047.191148	237836.663144	54.024090
3046.976417	237700.643350	54.029095
3046.232145	237549.123648	54.034100
3045.513145	237396.352433	54.039105
3044.624269	237253.055395	54.044109
3044.167573	237100.166696	54.049114
3043.439331	236960.791513	54.054119
3042.870802	236814.796136	54.059124
3042.031475	236669.887834	54.064129
3041.412778	236528.993529	54.069133
3040.648030	236375.288878	54.074138
3040.136836	236241.609607	54.079143
3039.650539	236087.784918	54.084148
3038.836597	235938.341111	54.089153
3038.009034	235800.129060	54.094157
3037.499270	235640.452160	54.099162
3036.431348	235501.794752	54.104167
3036.145626	235357.895593	54.109172
3035.470728	235214.338334	54.114177
3034.639436	235068.005073	54.119181
3034.198624	234925.633411	54.124186
3033.208262	234788.747133	54.129191
3032.792219	234638.351051	54.134196
3032.048053	234497.479414	54.139201
3031.483503	234353.702219	54.144205
3030.560852	234209.650895	54.149210
3029.903182	234066.398118	54.154215
3029.681360	233923.611285	54.159220
3029.140594	233773.312651	54.164225
3028.392503	233623.989193	54.169229
3028.097842	233477.980753	54.174234
3026.913720	233328.497601	54.179239
3026.315455	233179.991386	54.184244
3025.866702	233030.876091	54.189249
3024.768276	232887.134642	54.194253
3024.188116	232733.177235	54.199258
3023.371595	232587.176365	54.204263
3022.848919	232431.478890	54.209268
3022.165707	232286.832362	54.214273
3021.148696	232143.410168	54.219277
3020.825505	232001.126031	54.224282
3019.901827	231856.874704	54.229287
3019.640394	231708.877653	54.234292
3018.985958	231568.352589	54.239297
3017.935089	231430.462182	54.244301
3017.526293	231274.824995	54.249306
3016.729299	231134.450468	54.254311
3016.339990	230991.338094	54.259316
3015.542159	230849.105397	54.264321
3014.977258	230705.359250	54.269325
3014.692374	230557.775158	54.274330
3013.421249	230429.876795	54.279335
3013.068216	230276.371296	54.284340
3012.238684	230140.790310	54.289345
3011.474722	229995.600010	54.294349
3011.028716	229844.299691	54.299354
3010.121712	229699.998218	54.304359
3009.425330	229555.969181	54.309364
3008.654900	229409.940622	54.314369
3008.275320	229272.838415	54.319373
3008.079088	229125.242657	54.324378
3006.991635	228980.181613	54.329383
3006.333427	228832.303013	54.334388
3006.052771	228683.371901	54.339393
3005.193358	228543.571485	54.344397
3004.601215	228393.493486	54.349402
3003.643038	228240.214630	54.354407
3003.060276	228092.248967	54.359412
3002.498059	227951.434936	54.364417
3001.791318	227814.386820	54.369421
3001.245827	227658.904931	54.374426
3000.208099	227522.673516	54.379431
2999.743806	227374.053815	54.384436
2999.022125	227224.533059	54.389441
2998.129269	227089.679770	54.394445
2997.474878	226939.232270	54.399450
2996.960494	226812.568883	54.404455
2996.441592	226662.011321	54.409460
2995.942754	226508.662889	54.414465
2995.074880	226365.481108	54.419469
2994.677932	226213.988462	54.424474
2993.790495	226073.483667	54.429479
2993.076244	225930.329244	54.434484
2992.257862	225781.832087	54.439489
2991.656713	225639.856918	54.444493
2991.099758	225497.429440	54.449498
2990.217772	225354.353501	54.454503
2989.631264	225204.012994	54.459508
2988.730024	225068.795163	54.464513
2988.205784	224933.912515	54.469517
2987.651304	224780.232417	54.474522
2986.620272	224650.344317	54.479527
2986.090708	224499.703319	54.484532
2985.523362	224373.688605	54.489537
2984.763733	224236.629357	54.494541
2984.021176	224083.120405	54.499546
2983.539291	223955.616140	54.504551
2982.680612	223809.305845	54.509556
2982.391554	223672.580442	54.514561
2981.659883	223537.733000	54.519565
2981.022828	223397.549695	54.524570
2980.177764	223255.731949	54.529575
2979.542783	223121.200898	54.534580
2978.859437	222978.403315	54.539585
2977.984907	222839.849843	54.544589
2977.723713	222709.232050	54.549594
2976.871404	222569.644429	54.554599
2976.818461	222415.202153	54.559604
2976.088029	222281.667870	54.564609
2974.949676	222139.516713	54.569613
2974.805345	221989.927063	54.574618
2974.074508	221848.870341	54.579623
2973.138742	221708.431887	54.584628
2972.655553	221564.154074	54.589633
2971.799293	221424.963796	54.594637
2971.219857	221260.919972	54.599642
2970.574987	221140.192857	54.604647
2969.390440	220989.700581	54.609652
2968.891812	220865.704724	54.614657
2968.125254	220725.508644	54.619661
2967.721497	220576.332030	54.624666
2967.019069	220439.970639	54.629671
2966.197318	220299.364031	54.634676
2965.619180	220172.288671	54.639681
2965.149343	220033.549000	54.644685
2964.493243	219890.371073	54.649690
2963.756041	219743.374737	54.654695
2963.300132	219598.599981	54.659700
2962.435843	219475.440842	54.664705
2961.755765	219330.982152	54.669709
2961.221465	219187.697220	54.674714
2960.389063	219053.255650	54.679719
2959.591570	218898.543940	54.684724
2958.993828	218764.842239	54.689729
2958.359568	218628.142492	54.694733
2957.455580	218496.819206	54.699738
2956.956585	218369.696291	54.704743
2956.230324	218223.757836	54.709748
2955.467934	218088.034090	54.714753
2954.896311	217958.695826	54.719757
2954.386678	217812.583903	54.724762
2953.699653	217684.995553	54.729767
2952.945653	217547.247612	54.734772
2952.257437	217410.813334	54.739777
2951.681774	217272.566729	54.744781
2950.998108	217126.114649	54.749786
2950.475779	216996.757624	54.754791
2949.821089	216849.690553	54.759796
2949.470611	216722.127053	54.764801
2948.260580	216587.355371	54.769805
2947.922719	216438.800663	54.774810
2946.753375	216308.885463	54.779815
2946.050653	216165.009634	54.784820
2945.585004	216029.459304	54.789825
2944.776352	215896.827491	54.794829
2944.415540	215766.759857	54.799834
2943.281318	215635.732987	54.804839
2942.881218	215494.330921	54.809844
2942.278272	215368.019125	54.814849
2941.380293	215242.199773	54.819853
2941.336601	215097.636350	54.824858
2940.402222	214966.146370	54.829863
2939.925637	214830.269228	54.834868
2939.218879	214699.469254	54.839873
2938.344541	214559.187962	54.844877
2937.991355	214418.226222	54.849882
2937.055572	214293.292893	54.854887
2936.388112	214150.637694	54.859892
2935.618810	214010.531853	54.864897
2934.543096	213891.947392	54.869901
2934.025730	213750.796683	54.874906
2933.715857	213625.129108	54.879911
2932.780866	213490.892852	54.884916
2932.153755	213368.038011	54.889921
2931.750339	213233.603567	54.894925
2931.392287	213089.387033	54.899930
2930.403065	212967.112129	54.904935
2930.030585	212824.069450	54.909940
2929.763111	212681.837781	54.914945
2928.785825	212546.515557	54.919949
2928.077423	212396.361144	54.924954
2927.233007	212253.508997	54.929959
2926.229291	212122.519347	54.934964
2925.688527	212001.829897	54.939969
2924.974236	211865.016488	54.944973
2924.463983	211731.340299	54.949978
2923.787862	211608.191094	54.954983
2923.121900	211467.145253	54.959988
2922.472638	211329.648125	54.964993
2921.564388	211197.041565	54.969997
2921.202909	211056.190256	54.975002
2920.661168	210932.626529	54.980007
2920.001707	210794.928536	54.985012
2919.276187	210655.115790	54.990017
2918.741012	210510.958566	54.995021
2918.251896	210372.890883	55.000026
2917.071982	210247.507685	55.005031
2916.452095	210116.970521	55.010036
2915.740313	209974.560711	55.015041
2915.029393	209847.780405	55.020045
2914.576203	209711.108522	55.025050
2913.616951	209587.524470	55.030055
2913.166356	209445.049070	55.035060
2912.523537	209313.549950	55.040065
2911.464087	209178.782520	55.045069
2910.965802	209054.655642	55.050074
2910.444247	208922.527250	55.055079
2909.824658	208799.743732	55.060084
2909.447215	208655.553132	55.065089
2908.609571	208528.350163	55.070093
2907.846329	208395.013918	55.075098
2907.039257	208266.648486	55.080103
2906.469547	208131.016751	55.085108
2905.953314	207991.482369	55.090113
2905.197237	207868.633258	55.095117
2904.703228	207730.546845	55.100122
2903.535976	207605.612510	55.105127
2903.003238	207466.654674	55.110132
2902.610001	207344.550984	55.115137
2901.866627	207213.772325	55.120141
2901.330804	207074.484991	55.125146
2900.397283	206950.316814	55.130151
2900.111355	206813.599528	55.135156
2899.131718	206685.964784	55.140161
2898.477511	206561.180491	55.145165
2898.043091	206419.371469	55.150170
2897.465846	206283.312419	55.155175
2896.649512	206145.891607	55.160180
2896.042373	206015.641275	55.165185
2895.096566	205890.090073	55.170189
2894.433739	205752.696784	55.175194
2893.523448	205625.384259	55.180199
2893.211237	205492.784887	55.185204
2892.357559	205364.344034	55.190209
2891.549180	205246.268373	55.195213
2891.375401	205105.172132	55.200218
2890.129753	204985.740878	55.205223
2889.795635	204857.511591	55.210228
2889.255963	204729.786012	55.215233
2888.824368	204603.812565	55.220237
2887.881238	204460.498077	55.225242
2886.925269	204336.020869	55.230247
2886.631221	204202.887082	55.235252
2885.981359	204074.760445	55.240257
2885.143331	203949.641821	55.245261
2884.679204	203818.444791	55.250266
2884.094884	203698.224299	55.255271
2883.186361	203557.070048	55.260276
2882.633137	203423.597342	55.265281
2881.880724	203303.569744	55.270285
2881.360190	203171.352337	55.275290
2880.403254	203048.417959	55.280295
2879.898008	202915.613337	55.285300
2879.294362	202789.607532	55.290305
2878.654021	202651.505490	55.295309
2878.018748	202522.654694	55.300314
2877.389399	202396.742926	55.305319
2876.914729	202260.257252	55.310324
2876.130113	202128.275016	55.315329
2875.584076	201990.859598	55.320333
2875.181501	201852.340119	55.325338
2873.897998	201727.831477	55.330343
2873.308005	201600.617267	55.335348
2872.908099	201469.975507	55.340353
2871.979373	201337.623487	55.345357
2871.594952	201202.958622	55.350362
2870.500377	201066.166847	55.355367
2870.233327	200941.091819	55.360372
2869.120979	200815.578285	55.365377
2868.625961	200691.799751	55.370381
2868.211718	200556.581283	55.375386
2867.161594	200429.582639	55.380391
2866.160923	200297.868081	55.385396
2866.100548	200169.300806	55.390401
2865.057702	200049.478986	55.395405
2864.552632	199922.153445	55.400410
2863.964439	199801.687545	55.405415
2863.476637	199673.278213	55.410420
2862.882444	199539.974117	55.415425
2861.984322	199412.762925	55.420429
2861.567728	199279.265928	55.425434
2860.558732	199158.982635	55.430439
2859.787939	199031.917615	55.435444
2859.090649	198905.681110	55.440449
2858.380990	198783.149837	55.445453
2857.808427	198652.211386	55.450458
2857.287229	198527.436717	55.455463
2856.600199	198397.585917	55.460468
2855.958530	198276.101220	55.465473
2855.169093	198162.287834	55.470477
2854.827231	198030.919921	55.475482
2853.966224	197902.090429	55.480487
2853.351194	197774.736548	55.485492
2852.545623	197638.391323	55.490497
2852.016129	197515.567253	55.495501
2851.658291	197388.364455	55.500506
2850.780514	197266.804966	55.505511
2849.820315	197136.020756	55.510516
2849.541857	197010.765899	55.515521
2848.631994	196888.334383	55.520525
2848.068743	196754.014480	55.525530
2847.358039	196638.181484	55.530535
2846.479756	196515.554984	55.535540
2846.312046	196384.201823	55.540545
2845.273796	196259.552636	55.545549
2844.588399	196131.094191	55.550554
2844.108196	196005.084815	55.555559
2843.516817	195879.576878	55.560564
2842.914175	195760.484058	55.565569
2841.942464	195630.316265	55.570573
2841.990621	195497.149802	55.575578
2840.643957	195378.621046	55.580583
2840.188351	195242.315815	55.585588
2839.582133	195119.267860	55.590593
2838.741376	194998.776711	55.595597
2837.940294	194866.433491	55.600602
2837.153190	194749.891614	55.605607
2836.839228	194620.831034	55.610612
2836.092239	194494.905829	55.615617
2835.381282	194378.938055	55.620621
2834.922992	194246.733038	55.625626
2833.837130	194118.546700	55.630631
2833.297536	193997.997534	55.635636
2832.912047	193869.548235	55.640641
2831.788290	193743.035678	55.645645
2831.084340	193620.248628	55.650650
2830.905775	193506.641521	55.655655
2830.123891	193380.381116	55.660660
2829.740860	193256.997025	55.665665
2828.550458	193136.260374	55.670669
2828.290935	193008.722175	55.675674
2827.399630	192894.758576	55.680679
2826.770151	192768.831858	55.685684
2825.978289	192637.052939	55.690689
2825.218854	192518.183520	55.695693
2824.783250	192388.639066	55.700698
2824.126764	192272.324066	55.705703
2823.225246	192144.431743	55.710708
2822.822933	192028.369708	55.715713
2821.921686	191908.226455	55.720717
2821.537970	191781.538131	55.725722
2820.800576	191653.124900	55.730727
2819.840752	191528.398787	55.735732
2819.741390	191406.348537	55.740737
2818.831030	191288.142181	55.745741
2818.268028	191161.814672	55.750746
2817.225590	191043.871571	55.755751
2816.716605	190920.297042	55.760756
2815.940429	190798.686315	55.765761
2815.605803	190689.754365	55.770765
2815.067711	190562.673830	55.775770
2814.293654	190435.363822	55.780775
2813.360217	190309.580691	55.785780
2813.065011	190187.297371	55.790785
2811.981263	190062.467463	55.795789
2811.805178	189926.361726	55.800794
2810.861974	189812.273664	55.805799
2810.515609	189689.198195	55.810804
2809.700175	189564.479775	55.815809
2808.748401	189447.111506	55.820813
2808.427444	189313.116982	55.825818
2807.454337	189196.134394	55.830823
2806.662746	189071.031826	55.835828
2806.383164	188949.538021	55.840833
2805.452811	188840.475657	55.845837
2804.809889	188706.279402	55.850842
2803.779873	188592.869609	55.855847
2803.096328	188467.611592	55.860852
2802.991857	188347.071236	55.865857
2801.873088	188235.342992	55.870861
2801.652499	188105.928767	55.875866
2800.831873	187996.685607	55.880871
2800.267824	187873.331318	55.885876
2799.732018	187748.535279	55.890881
2799.211619	187629.843758	55.895885
2798.587868	187497.976098	55.900890
2797.509471	187379.640757	55.905895
2797.142257	187255.646281	55.910900
2796.508690	187128.017668	55.915905
2795.397630	187010.337271	55.920909
2794.952801	186888.684194	55.925914
2794.252217	186774.285258	55.930919
2793.753395	186637.973058	55.935924
2793.035369	186513.679934	55.940929
2792.478107	186398.266937	55.945933
2791.934109	186276.542140	55.950938
2791.097422	186165.423053	55.955943
2790.577197	186034.624551	55.960948
2789.884695	185898.625113	55.965953
2789.014633	185780.464461	55.970957
2788.423598	185653.609251	55.975962
2787.865850	185522.678230	55.980967
2787.033490	185402.540755	55.985972
2786.292362	185280.112008	55.990977
2785.506533	185173.427096	55.995981
2785.074635	185039.131806	56.000986
2784.105218	184924.983654	56.005991
2783.577601	184800.423369	56.010996
2783.030984	184675.840996	56.016001
2782.221867	184563.131327	56.021005
2781.787853	184436.445497	56.026010
2781.327481	184320.259192	56.031015
2780.145797	184190.779326	56.036020
2779.674804	184068.145730	56.041025
2779.044011	183945.855810	56.046029
2778.432071	183823.817662	56.051034
2777.619293	183709.813185	56.056039
2776.816932	183588.174756	56.061044
2776.531188	183472.382802	56.066049
2775.681709	183358.257835	56.071053
2775.278645	183232.321073	56.076058
2774.451076	183109.441309	56.081063
2773.889311	182992.842035	56.086068
2773.341299	182869.816895	56.091073
2772.085654	182754.180451	56.096077
2771.918199	182620.779204	56.101082
2770.925204	182505.559761	56.106087
2770.422503	182382.172635	56.111092
2769.916284	182265.998999	56.116097
2768.845083	182145.284872	56.121101
2768.315103	182023.785725	56.126106
2767.724657	181913.108924	56.131111
2766.938373	181791.638302	56.136116
2766.596074	181667.629932	56.141121
2765.865523	181553.796131	56.146125
2765.174181	181418.764291	56.151130
2764.545600	181308.273161	56.156135
2763.802917	181180.271820	56.161140
2763.404360	181066.361278	56.166145
2762.344310	180951.385553	56.171149
2761.815831	180823.898313	56.176154
2761.140622	180700.784985	56.181159
2760.565062	180585.771659	56.186164
2759.834006	180463.990749	56.191169
2759.179816	180346.624585	56.196173
2758.706733	180220.402372	56.201178
2758.085634	180113.029536	56.206183
2757.142478	179983.842406	56.211188
2756.700290	179858.417727	56.216193
2755.906379	179736.089176	56.221197
2755.294508	179610.374109	56.226202
2754.890368	179485.555056	56.231207
2754.039431	179371.364536	56.236212
2753.388566	179265.919241	56.241217
2752.605317	179134.356223	56.246221
2752.207354	178998.942134	56.251226
2751.226469	178892.545195	56.256231
2750.722652	178761.587780	56.261236
2750.334641	178634.275654	56.266241
2749.319343	178516.793689	56.271245
2748.487905	178391.905644	56.276250
2747.773173	178264.290249	56.281255
2747.236536	178148.641411	56.286260
2746.707416	178019.102176	56.291265
2745.829968	177901.333000	56.296269
2745.413643	177773.112190	56.301274
2744.516654	177667.430079	56.306279
2743.627421	177553.136109	56.311284
2743.184801	177424.691593	56.316289
2742.604622	177308.670412	56.321293
2742.010124	177193.058836	56.326298
2741.109854	177082.367416	56.331303
2740.598341	176950.615611	56.336308
2740.066599	176833.863106	56.341313
2739.231325	176719.893586	56.346317
2738.658339	176602.397854	56.351322
2738.018899	176486.655469	56.356327
2737.509090	176358.606481	56.361332
2736.835298	176234.183287	56.366337
2735.774660	176114.184283	56.371341
2735.112200	175993.270405	56.376346
2734.571372	175876.547501	56.381351
2734.186494	175768.995813	56.386356
2733.244958	175642.645442	56.391361
2732.501071	175526.159206	56.396365
2731.916339	175410.856354	56.401370
2731.611547	175286.542941	56.406375
2730.680309	175167.162157	56.411380
2730.030472	175047.202976	56.416385
2729.439557	174933.772068	56.421389
2728.557140	174809.945888	56.426394
2727.901691	174701.638633	56.431399
2727.265430	174578.664452	56.436404
2727.082582	174452.439263	56.441409
2725.881768	174340.213125	56.446413
2725.613938	174216.901887	56.451418
2725.147834	174104.738078	56.456423
2724.281257	173968.855195	56.461428
2723.680987	173853.991671	56.466433
2722.896430	173724.710011	56.471437
2722.553117	173605.584118	56.476442
2721.766671	173487.940468	56.481447
2721.285121	173353.499403	56.486452
2720.526722	173237.200147	56.491457
2719.800889	173114.766087	56.496461
2719.125677	172982.633443	56.501466
2718.210424	172859.212756	56.506471
2717.631646	172738.753246	56.511476
2716.927546	172615.973906	56.516481
2716.349562	172499.330296	56.521485
2715.873395	172374.925897	56.526490
2714.964431	172245.770506	56.531495
2714.534294	172128.010866	56.536500
2714.186198	172003.650939	56.541505
2713.209673	171876.084429	56.546509
2712.487627	171753.615841	56.551514
2711.650161	171618.842825	56.556519
2710.978021	171495.273449	56.561524
2710.369199	171367.802955	56.566529
2709.924833	171252.222850	56.571533
2709.458394	171126.892513	56.576538
2708.503486	171010.452933	56.581543
2708.075239	170874.218778	56.586548
2707.043949	170745.189461	56.591553
2706.010545	170636.279213	56.596557
2705.588542	170501.240778	56.601562
2705.079842	170391.764852	56.606567
2704.245958	170262.286213	56.611572
2703.732847	170142.600032	56.616577
2703.074763	170015.332538	56.621581
2702.604702	169896.784813	56.626586
2701.907942	169786.183172	56.631591
2700.661996	169660.078186	56.636596
2700.386717	169525.617607	56.641601
2699.465098	169413.310483	56.646605
2699.053418	169298.977268	56.651610
2698.394919	169179.889364	56.656615
2697.595898	169050.867082	56.661620
2697.143328	168939.656959	56.666625
2696.195996	168816.266921	56.671629
2695.836866	168694.945883	56.676634
2695.104832	168582.763765	56.681639
2694.324142	168460.429370	56.686644
2693.905617	168338.343185	56.691649
2693.009716	168213.433724	56.696653
2692.589493	168088.919815	56.701658
2691.979591	167967.615397	56.706663
2691.329787	167847.932632	56.711668
2690.819160	167720.191658	56.716673
2690.132599	167595.492681	56.721677
2689.708790	167458.278139	56.726682
2688.548055	167336.579809	56.731687
2687.987216	167216.706934	56.736692
2687.547325	167087.596303	56.741697
2686.570904	166968.336841	56.746701
2686.043174	166847.137460	56.751706
2685.345754	166725.164265	56.756711
2684.966089	166586.814220	56.761716
2684.134778	166466.795862	56.766721
2683.099064	166349.785718	56.771725
2682.776613	166221.778444	56.776730
2682.303096	166097.330451	56.781735
2681.338334	165967.353187	56.786740
2680.875271	165843.349429	56.791745
2680.156773	165723.315600	56.796749
2679.698683	165586.151518	56.801754
2678.905465	165466.054070	56.806759
2678.269163	165339.167649	56.811764
2677.679364	165212.554032	56.816769
2676.810679	165088.528062	56.821773
2676.256906	164956.785415	56.826778
2675.651508	164829.412681	56.831783
2674.738198	164703.551399	56.836788
2674.226753	164578.415209	56.841793
2673.537339	164458.813204	56.846797
2672.558394	164325.398240	56.851802
2672.407131	164207.186725	56.856807
2671.664639	164079.151721	56.861812
2670.858307	163943.956162	56.866817
2670.066735	163822.706796	56.871821
2669.768947	163689.936408	56.876826
2668.848098	163569.305958	56.881831
2668.158660	163437.272418	56.886836
2667.520017	163312.771025	56.891841
2666.656536	163185.978932	56.896845
2666.033267	163063.230560	56.901850
2665.002076	162943.357116	56.906855
2664.590565	162813.316124	56.911860
2664.131116	162695.832218	56.916865
2663.560922	162579.052811	56.921869
2662.901436	162451.124840	56.926874
2662.218357	162323.277348	56.931879
2661.598030	162204.243978	56.936884
2661.131851	162073.820184	56.941889
2660.085622	161946.756273	56.946893
2659.653773	161818.146079	56.951898
2658.879483	161693.353933	56.956903
2658.037161	161572.145610	56.961908
2657.797956	161444.536067	56.966913
2656.881202	161327.853791	56.971917
2656.397071	161198.376861	56.976922
2655.966162	161077.753442	56.981927
2654.825277	160951.496331	56.986932
2654.514858	160816.030553	56.991937
2653.515655	160689.764641	56.996941
2652.719814	160556.385514	57.001946
2652.186161	160436.263673	57.006951
2651.559946	160310.588410	57.011956
2651.192279	160191.165771	57.016961
2650.065611	160072.219767	57.021965
2649.725463	159947.403125	57.026970
2649.190518	159819.248769	57.031975
2648.637771	159696.170283	57.036980
2647.916009	159564.486751	57.041985
2647.247267	159440.079944	57.046989
2646.781679	159305.725175	57.051994
2645.868534	159185.578745	57.056999
2644.983783	159050.579440	57.062004
2644.617340	158913.693296	57.067009
2643.482495	158794.714793	57.072013
2643.350106	158663.627774	57.077018
2642.775569	158537.315044	57.082023
2641.982860	158416.821653	57.087028
2641.177599	158280.312636	57.092033
2640.229569	158153.018041	57.097037
2639.817438	158021.558251	57.102042
2639.029339	157900.366732	57.107047
2638.744273	157765.353686	57.112052
2638.330838	157635.878725	57.117057
2637.072433	157513.364711	57.122061
2636.608037	157381.648678	57.127066
2636.103739	157254.706601	57.132071
2635.235439	157127.428586	57.137076
2634.811412	156997.754308	57.142081
2633.849771	156871.763257	57.147085
2633.463787	156739.516064	57.152090
2632.749231	156618.330128	57.157095
2632.099495	156483.405325	57.162100
2631.465908	156344.664895	57.167105
2630.598709	156225.779988	57.172109
2629.939242	156085.595550	57.177114
2629.470899	155958.029707	57.182119
2629.231912	155830.199189	57.187124
2628.219585	155692.856169	57.192129
2627.336320	155557.056797	57.197133
2626.872622	155429.352377	57.202138
2626.302245	155296.237483	57.207143
2625.453906	155164.476447	57.212148
2624.831143	155026.909156	57.217153
2624.021309	154905.642741	57.222157
2623.555877	154777.458027	57.227162
2622.735465	154655.965383	57.232167
2622.088969	154516.217584	57.237172
2621.661708	154383.388692	57.242177
2620.858544	154265.186949	57.247181
2620.784437	154115.295547	57.252186
2619.661554	153987.917137	57.257191
2619.029573	153852.478876	57.262196
2618.380785	153709.353665	57.267201
2617.658455	153580.693084	57.272205
2616.886333	153449.282621	57.277210
2616.235188	153314.752058	57.282215
2615.666628	153183.971354	57.287220
2615.240619	153056.791144	57.292225
2614.338016	152922.289305	57.297229
2613.519473	152782.423505	57.302234
2612.965305	152649.875846	57.307239
2612.113654	152516.397143	57.312244
2611.754322	152385.802517	57.317249
2610.565108	152256.458428	57.322253
2609.854388	152129.047272	57.327258
2609.621269	151991.773956	57.332263
2608.870993	151816.083676	57.337268
2608.455103	151680.492958	57.342273
2607.625924	151547.421353	57.347277
2607.197459	151397.738207	57.352282
2606.584938	151282.338558	57.357287
2605.705069	151152.276172	57.362292
2605.580059	151013.858626	57.367297
2604.325741	150878.785385	57.372301
2604.076228	150721.959423	57.377306
2603.343168	150607.191337	57.382311
2602.684893	150465.441680	57.387316
2601.906988	150336.688212	57.392321
2600.896318	150204.070273	57.397325
2600.664516	150064.834848	57.402330
2599.979173	149922.837661	57.407335
2599.364838	149794.606939	57.412340
2598.851405	149644.233596	57.417345
2597.924843	149511.821230	57.422349
2597.349153	149383.852914	57.427354
2596.796932	149238.469670	57.432359
2596.133132	149100.145674	57.437364
2595.302128	148954.960400	57.442369
2594.491379	148824.756618	57.447373
2594.052624	148685.115129	57.452378
2593.500263	148544.348441	57.457383
2592.798518	148404.749850	57.462388
2592.557399	148272.157732	57.467393
2591.533790	148132.369866	57.472397
2590.668685	147993.243772	57.477402
2590.053389	147857.789649	57.482407
2589.481520	147724.718453	57.487412
2588.856153	147583.268601	57.492417
2587.908222	147442.073831	57.497421
2587.373826	147296.023051	57.502426
2586.924188	147171.665552	57.507431
2585.976631	147032.429652	57.512436
2585.514781	146887.805311	57.517441
2584.813676	146752.941384	57.522445
2584.422196	146607.404888	57.527450
2583.331193	146476.645148	57.532455
2582.333653	146332.502197	57.537460
2582.156777	146202.056233	57.542465
2581.295978	146067.144305	57.547469
2581.155345	145924.316150	57.552474
2580.391102	145789.466364	57.557479
2579.250691	145642.312040	57.562484
2579.188930	145500.693271	57.567489
2577.950134	145364.408295	57.572493
2577.643323	145223.210849	57.577498
2576.891275	145099.938798	57.582503
2576.482369	144953.332600	57.587508
2575.897182	144813.655202	57.592513
2574.915995	144669.847729	57.597517
2574.717761	144523.629519	57.602522
2573.681265	144378.586839	57.607527
2572.920616	144223.983386	57.612532
2572.341650	144109.303368	57.617537
2571.813446	143963.368825	57.622541
2571.142856	143823.048657	57.627546
2570.230926	143681.306065	57.632551
2569.492395	143541.379159	57.637556
2569.249687	143391.272314	57.642561
2568.307689	143270.096182	57.647565
2567.872465	143125.269082	57.652570
2566.867536	142976.263482	57.657575
2566.369299	142840.621985	57.662580
2565.784462	142695.490252	57.667585
2565.226554	142545.208781	57.672589
2564.322436	142410.459441	57.677594
2563.792791	142273.021117	57.682599
2563.017020	142132.051921	57.687604
2562.519125	141987.163908	57.692609
2561.722533	141844.611052	57.697613
2560.995501	141707.981645	57.702618
2560.476749	141560.316313	57.707623
2559.623283	141425.792024	57.712628
2558.887164	141288.568762	57.717633
2558.146237	141150.508290	57.722637
2557.577548	141006.614545	57.727642
2556.854687	140871.208026	57.732647
2556.147060	140741.491903	57.737652
2555.687895	140592.995978	57.742657
2554.782061	140470.338717	57.747661
2554.517261	140322.499432	57.752666
2553.825354	140188.996924	57.757671
2553.056053	140042.077541	57.762676
2552.442587	139896.036270	57.767681
2551.917934	139766.752759	57.772685
2551.483425	139610.316918	57.777690
2550.564602	139471.123469	57.782695
2549.893543	139336.706682	57.787700
2549.452042	139192.128110	57.792705
2548.616601	139052.300852	57.797709
2547.745699	138909.938865	57.802714
2547.185630	138768.697156	57.807719
2546.468375	138623.021607	57.812724
2545.802830	138482.788959	57.817729
2545.283662	138338.366606	57.822733
2544.502824	138194.634369	57.827738
2543.916293	138063.500477	57.832743
2543.052466	137918.601202	57.837748
2543.033841	137769.211029	57.842753
2542.028182	137631.640757	57.847757
2541.411036	137490.642883	57.852762
2540.880921	137340.954812	57.857767
2539.989908	137204.143339	57.862772
2539.744628	137056.177476	57.867777
2538.679034	136917.552894	57.872781
2538.023470	136769.145338	57.877786
2537.741882	136637.435909	57.882791
2536.657891	136491.701993	57.887796
2536.263054	136324.644031	57.892801
2535.441135	136185.107738	57.897805
2534.913315	136040.113685	57.902810
2534.416531	135894.365916	57.907815
2533.387251	135751.434560	57.912820
2532.907911	135601.772765	57.917825
2532.049422	135462.664957	57.922829
2531.464518	135309.159526	57.927834
2531.178912	135171.689993	57.932839
2530.060373	135032.130037	57.937844
2529.633333	134875.769039	57.942849
2528.967392	134736.913680	57.947853
2528.299846	134586.740728	57.952858
2527.627895	134440.748576	57.957863
2527.154997	134291.994465	57.962868
2526.558383	134140.643922	57.967873
2525.803846	133997.893662	57.972877
2525.147594	133845.017080	57.977882
2524.444979	133695.502193	57.982887
2523.747149	133544.996518	57.987892
2523.269042	133377.905290	57.992897
2522.445136	133244.645941	57.997901
2521.941558	133097.401803	58.002906
2521.222566	132953.977892	58.007911
2520.349340	132796.073047	58.012916
2520.053868	132633.593601	58.017921
2519.039277	132504.229440	58.022925
2518.429920	132350.375372	58.027930
2517.647164	132202.329076	58.032935
2517.162141	132055.760609	58.037940
2516.559649	131908.398594	58.042945
2515.359759	131756.660964	58.047949
2515.178053	131603.111536	58.052954
2514.150801	131464.240476	58.057959
2513.583361	131325.678276	58.062964
2513.254043	131168.255191	58.067969
2512.260433	131033.445450	58.072973
2511.748159	130870.070595	58.077978
2511.046678	130725.842328	58.082983
2510.325670	130586.203093	58.087988
2509.852686	130432.071162	58.092993
2509.081308	130283.753733	58.097997
2508.637515	130142.281904	58.103002
2507.762881	129991.658080	58.108007
2507.326106	129840.813259	58.113012
2506.810691	129696.611621	58.118017
2505.580814	129558.582301	58.123021
2505.228802	129401.833208	58.128026
2504.706271	129251.551311	58.133031
2503.918687	129102.213988	58.138036
2503.114150	128944.192932	58.143041
2502.496498	128798.665901	58.148045
2501.634515	128649.571425	58.153050
2501.220763	128504.508943	58.158055
2500.443343	128359.809674	58.163060
2500.281257	128202.834064	58.168065
2499.145371	128061.253949	58.173069
2498.539483	127901.061048	58.178074
2498.142415	127756.990470	58.183079
2497.379776	127613.677093	58.188084
2496.915424	127460.931932	58.193089
2495.867046	127308.064295	58.198093
2495.383076	127144.427526	58.203098
2494.368423	127009.856614	58.208103
2493.908955	126868.480245	58.213108
2493.387651	126707.049056	58.218113
2492.669810	126562.159345	58.223117
2492.108654	126409.244917	58.228122
2491.489060	126258.004229	58.233127
2490.732405	126111.319761	58.238132
2490.174368	125951.194210	58.243137
2489.493800	125806.734395	58.248141
2489.204086	125643.177455	58.253146
2488.306090	125493.178877	58.258151
2487.493242	125341.046912	58.263156
2487.055554	125194.215264	58.268161
2486.389323	125038.061621	58.273165
2485.700627	124885.328402	58.278170
2484.931846	124723.326025	58.283175
2484.197366	124578.106715	58.288180
2483.760284	124421.628260	58.293185
2482.823223	124274.639514	58.298189
2482.344245	124108.531409	58.303194
2481.454048	123963.670267	58.308199
2480.987178	123814.222240	58.313204
2480.582063	123651.825842	58.318209
2479.578211	123502.337696	58.323213
2479.046279	123342.744160	58.328218
2478.535136	123189.776603	58.333223
2477.532302	123028.773935	58.338228
2477.066159	122878.251722	58.343233
2476.497741	122728.965553	58.348237
2475.603518	122560.279095	58.353242
2474.846027	122418.148018	58.358247
2474.357546	122271.492847	58.363252
2473.891607	122108.810779	58.368257
2472.921712	121961.700346	58.373261
2472.430069	121807.353665	58.378266
2471.968368	121643.886559	58.383271
2470.913535	121487.396320	58.388276
2470.343559	121339.895842	58.393281
2469.538758	121186.389658	58.398285
2469.058559	121023.475308	58.403290
2468.414054	120875.811494	58.408295
2467.682172	120717.446311	58.413300
2467.178523	120561.331308	58.418305
2466.319176	120407.400298	58.423309
2465.601019	120259.504054	58.428314
2464.783916	120099.696023	58.433319
2464.413301	119940.738683	58.438324
2463.517681	119788.061323	58.443329
2462.798872	119644.929778	58.448333
2461.958823	119497.425374	58.453338
2461.668827	119347.549320	58.458343
2460.896144	119199.210687	58.463348
2460.418890	119039.393390	58.468353
2459.504845	118904.682536	58.473357
2458.930587	118737.518884	58.478362
2458.592049	118587.477181	58.483367
2457.465385	118444.410575	58.488372
2457.060622	118280.999960	58.493377
2456.596228	118124.842600	58.498381
2455.930694	117970.412907	58.503386
2455.459851	117815.286774	58.508391
2454.591093	117678.873976	58.513396
2454.093666	117515.927242	58.518401
2453.414640	117358.221667	58.523405
2452.471973	117189.488803	58.528410
2452.046371	117035.191740	58.533415
2451.257582	116892.613411	58.538420
2450.909972	116728.867204	58.543425
2450.118944	116580.946468	58.548429
2449.231778	116403.761670	58.553434
2448.887829	116246.974630	58.558439
2448.073317	116097.797317	58.563444
2447.444094	115938.410605	58.568449
2446.988363	115774.192596	58.573453
2445.985168	115616.657087	58.578458
2445.567552	115465.294292	58.583463
2444.677217	115296.089657	58.588468
2444.266294	115136.470279	58.593473
2443.249515	114991.431705	58.598477
2442.961946	114821.722141	58.603482
2441.975067	114667.007998	58.608487
2441.143741	114505.897923	58.613492
2440.848545	114355.252264	58.618497
2439.708464	114189.045914	58.623501
2439.439829	114043.767266	58.628506
2438.594942	113890.114340	58.633511
2437.831747	113731.391133	58.638516
2437.678762	113577.693903	58.643521
2436.687487	113430.959410	58.648525
2436.236773	113254.838193	58.653530
2435.816841	113097.676607	58.658535
2434.845822	112937.766518	58.663540
2434.471867	112776.544295	58.668545
2433.726670	112623.080099	58.673549
2432.975488	112461.824522	58.678554
2432.172626	112295.171159	58.683559
2431.779341	112132.642498	58.688564
2431.075195	111976.351719	58.693569
2430.165455	111827.354520	58.698573
2429.570174	111651.058160	58.703578
2428.722380	111494.425125	58.708583
2428.133543	111343.983832	58.713588
2427.683528	111182.479426	58.718593
2427.021739	111034.513830	58.723597
2426.732334	110867.039875	58.728602
2426.107793	110686.382720	58.733607
2425.140325	110536.837692	58.738612
2424.751735	110367.237978	58.743617
2424.103330	110220.258759	58.748621
2423.426918	110047.007323	58.753626
2422.328427	109875.518318	58.758631
2421.662115	109711.341941	58.763636
2421.059226	109547.270834	58.768641
2420.383187	109386.600936	58.773645
2419.671814	109225.131824	58.778650
2419.187471	109067.600035	58.783655
2418.327374	108909.741767	58.788660
2418.017449	108735.299376	58.793665
2417.123232	108577.309081	58.798669
2416.374786	108413.953987	58.803674
2415.638012	108262.279711	58.808679
2415.116423	108096.251179	58.813684
2414.268438	107935.078807	58.818689
2413.865967	107776.584309	58.823693
2413.333440	107620.896952	58.828698
2412.702391	107457.091904	58.833703
2411.858241	107301.379875	58.838708
2411.680106	107125.284855	58.843713
2410.370104	106969.642486	58.848717
2409.803941	106801.237917	58.853722
2409.566874	106637.617093	58.858727
2408.725730	106478.636005	58.863732
2407.966088	106297.982191	58.868737
2406.694494	106145.416276	58.873741
2406.253245	105977.644850	58.878746
2405.966540	105819.297188	58.883751
2404.678590	105664.065874	58.888756
2404.870928	105499.388666	58.893761
2403.865600	105345.649989	58.898765
2403.234251	105178.637594	58.903770
2402.453583	105012.411371	58.908775
2401.889077	104847.807911	58.913780
2401.163722	104696.465272	58.918785
2400.533641	104534.424787	58.923789
2399.889157	104361.114054	58.928794
2399.307783	104208.349642	58.933799
2398.267693	104049.898489	58.938804
2397.670720	103902.670595	58.943809
2396.818148	103747.401846	58.948813
2396.448827	103575.632919	58.953818
2396.062397	103424.168571	58.958823
2395.410149	103266.409784	58.963828
2395.110083	103084.641817	58.968833
2393.943123	102936.749075	58.973837
2393.489939	102762.791737	58.978842
2392.752762	102601.967814	58.983847
2392.238712	102448.423882	58.988852
2391.650278	102257.084692	58.993857
2391.014082	102098.151312	58.998861
2390.248970	101940.336887	59.003866
2389.385334	101766.946834	59.008871
2388.382788	101612.324995	59.013876
2387.940117	101451.202228	59.018881
2387.361052	101291.916405	59.023885
2386.616389	101128.135141	59.028890
2386.023207	100966.519447	59.033895
2385.165631	100821.464585	59.038900
2384.690573	100645.116097	59.043905
2384.047203	100485.249753	59.048909
2382.967564	100331.359114	59.053914
2382.631751	100165.103119	59.058919
2382.156939	100002.137010	59.063924
2381.795678	99840.099153	59.068929
2380.631011	99678.944624	59.073933
2379.919733	99520.224778	59.078938
2379.391154	99350.700583	59.083943
2378.566406	99195.946210	59.088948
2378.248137	99029.981058	59.093953
2377.165770	98877.185193	59.098957
2376.901739	98700.856192	59.103962
2376.089423	98550.398187	59.108967
2375.382254	98396.112617	59.113972
2375.055154	98221.065830	59.118977
2374.355993	98059.652272	59.123981
2373.402077	97892.115407	59.128986
2373.342459	97730.774021	59.133991
2372.186584	97570.165721	59.138996
2371.671155	97398.884408	59.144001
2371.064773	97228.050080	59.149005
2370.394832	97062.364296	59.154010
2369.766846	96904.917869	59.159015
2368.890047	96732.360693	59.164020
2368.256191	96568.213935	59.169025
2367.650537	96411.915312	59.174029
2367.527198	96240.364961	59.179034
2366.405142	96066.069670	59.184039
2365.304799	95908.838263	59.189044
2364.809039	95729.036658	59.194049
2364.170077	95577.657674	59.199053
2363.636767	95419.794385	59.204058
2363.033964	95257.966984	59.209063
2362.194419	95092.728433	59.214068
2361.453755	94921.901159	59.219073
2360.982771	94759.530103	59.224077
2360.489105	94599.687740	59.229082
2359.779973	94436.044102	59.234087
2359.152666	94270.796995	59.239092
2358.547421	94103.968613	59.244097
2357.387256	93933.855890	59.249101
2357.261882	93765.419356	59.254106
2356.677229	93611.109067	59.259111
2355.922223	93447.086812	59.264116
2355.388603	93270.405478	59.269121
2354.413801	93117.904290	59.274125
2353.640411	92935.563011	59.279130
2353.488115	92766.098395	59.284135
2352.176760	92599.773737	59.289140
2351.691604	92440.211872	59.294145
2351.244818	92281.824471	59.299149
2350.510914	92113.978880	59.304154
2349.843187	91947.005438	59.309159
2349.420740	91769.234206	59.314164
2348.779521	91598.315293	59.319169
2347.818635	91439.799884	59.324173
2347.162088	91270.895920	59.329178
2346.466453	91106.285635	59.334183
2345.872132	90941.121582	59.339188
2345.437511	90766.213606	59.344193
2344.522786	90603.347411	59.349197
2343.924031	90429.311424	59.354202
2343.226721	90267.896887	59.359207
2342.640150	90116.610331	59.364212
2342.157512	89930.830507	59.369217
2341.127304	89765.072409	59.374221
2340.424741	89598.534512	59.379226
2340.358966	89427.237002	59.384231
2339.364023	89264.254060	59.389236
2338.584785	89094.682660	59.394241
2337.918121	88927.459507	59.399245
2337.205252	88752.225099	59.404250
2336.888598	88592.144731	59.409255
2336.231784	88431.238265	59.414260
2335.943046	88248.840189	59.419265
2335.005070	88088.240791	59.424269
2334.046664	87910.541655	59.429274
2333.621296	87732.930628	59.434279
2332.866086	87556.977255	59.439284
2332.058971	87402.251592	59.444289
2331.285700	87233.080581	59.449293
2330.902571	87052.660134	59.454298
2330.187452	86888.395593	59.459303
2329.534436	86717.428246	59.464308
2328.642357	86554.779131	59.469313
2327.994595	86386.476049	59.474317
2327.549581	86221.818804	59.479322
2327.111556	86038.461605	59.484327
2326.188693	85872.551636	59.489332
2325.539288	85706.136855	59.494337
2324.663546	85532.513939	59.499341
2324.221809	85361.042204	59.504346
2323.631313	85190.273690	59.509351
2322.934523	85023.903458	59.514356
2322.381443	84840.143801	59.519361
2321.213856	84684.962567	59.524365
2320.832562	84513.057075	59.529370
2320.444207	84348.107450	59.534375
2319.291387	84172.454244	59.539380
2319.114732	83995.696939	59.544385
2318.256045	83843.122361	59.549389
2317.614964	83664.793503	59.554394
2317.157434	83497.326175	59.559399
2316.180768	83320.695060	59.564404
2315.822687	83142.357444	59.569409
2315.007304	82972.263672	59.574413
2314.411739	82806.135730	59.579418
2313.589299	82633.643703	59.584423
2313.411190	82463.478352	59.589428
2312.604817	82290.371826	59.594433
2311.714031	82110.992981	59.599437
2311.144504	81937.268740	59.604442
2310.262938	81763.284880	59.609447
2309.258273	81603.581785	59.614452
2308.954233	81433.894770	59.619457
2308.486613	81259.310777	59.624461
2307.477687	81087.989195	59.629466
2307.231879	80913.081408	59.634471
2306.556641	80751.038456	59.639476
2305.961086	80567.494100	59.644481
2305.163969	80396.670641	59.649485
2304.238196	80226.711853	59.654490
2303.581561	80055.856257	59.659495
2302.897820	79894.873336	59.664500
2302.534128	79717.003207	59.669505
2301.593482	79560.252468	59.674509
2301.039396	79376.946583	59.679514
2300.159114	79214.244797	59.684519
2299.568871	79042.677332	59.689524
2298.778620	78880.242735	59.694529
2298.091288	78713.515762	59.699533
2297.604299	78536.530860	59.704538
2297.161298	78375.895518	59.709543
2296.276111	78206.320851	59.714548
2295.881340	78033.146671	59.719553
2295.011826	77863.553352	59.724557
2294.512059	77697.216786	59.729562
2293.589041	77524.466527	59.734567
2293.132871	77358.227194	59.739572
2292.359133	77173.341080	59.744577
2291.698290	77018.333268	59.749581
2291.193308	76849.938821	59.754586
2290.534069	76683.775220	59.759591
2289.348482	76515.181015	59.764596
2289.244553	76338.160778	59.769601
2288.146293	76177.665695	59.774605
2287.651048	76006.400157	59.779610
2287.165486	75842.306779	59.784615
2286.366508	75670.769121	59.789620
2285.848245	75506.316179	59.794625
2285.186612	75332.599105	59.799629
2284.538281	75158.076785	59.804634
2284.250841	74987.699271	59.809639
2283.374746	74823.226289	59.814644
2282.890785	74640.515817	59.819649
2282.108833	74473.179781	59.824653
2281.467461	74298.125306	59.829658
2280.885402	74127.421685	59.834663
2280.225468	73950.554938	59.839668
2279.578116	73771.476753	59.844673
2278.374401	73607.439486	59.849677
2277.918620	73429.486990	59.854682
2277.271586	73248.075776	59.859687
2276.386764	73082.560518	59.864692
2275.953399	72914.954175	59.869697
2275.199078	72747.007379	59.874701
2274.646032	72567.335899	59.879706
2273.764655	72411.606723	59.884711
2273.061438	72233.007329	59.889716
2272.698699	72060.107460	59.894721
2271.729387	71893.519599	59.899725
2271.220034	71736.267083	59.904730
2270.938936	71548.858812	59.909735
2269.997808	71386.381873	59.914740
2269.432200	71215.181196	59.919745
2268.438153	71039.324501	59.924750
2267.672088	70868.038275	59.929754
2267.371434	70706.535857	59.934759
2266.555570	70532.733067	59.939764
2266.483697	70350.250022	59.944769
2265.698506	70192.369469	59.949774
2264.812670	70013.559416	59.954778
2264.334519	69840.899985	59.959783
2263.539705	69666.430119	59.964788
2262.953177	69498.908716	59.969793
2262.437379	69314.681546	59.974798
2261.416721	69138.067038	59.979802
2260.990891	68964.760991	59.984807
2260.320084	68791.457333	59.989812
2259.853574	68612.422570	59.994817
2258.973702	68442.739990	59.999822
2258.191640	68270.218639	60.004826
2257.561265	68089.954304	60.009831
2256.968216	67917.393438	60.014836
2256.532349	67731.876539	60.019841
2255.788139	67566.284083	60.024846
2255.155941	67390.675144	60.029850
2254.529768	67209.063018	60.034855
2253.794560	67039.832077	60.039860
2253.488990	66855.281366	60.044865
2252.487505	66680.310585	60.049870
2251.701856	66492.087204	60.054874
2251.001942	66319.937502	60.059879
2250.300007	66150.230952	60.064884
2250.037977	65966.473436	60.069889
2248.904710	65792.237724	60.074894
2248.216596	65606.600762	60.079898
2247.470122	65444.525646	60.084903
2246.723782	65277.265552	60.089908
2246.299421	65096.217593	60.094913
2245.564732	64924.415198	60.099918
2244.894036	64752.341404	60.104922
2244.265955	64576.833469	60.109927
2243.505236	64407.689904	60.114932
2242.843811	64224.708975	60.119937
2242.125423	64062.549297	60.124942
2241.574633	63889.090197	60.129946
2241.103313	63718.725914	60.134951
2240.276809	63544.506356	60.139956
2240.086540	63355.605170	60.144961
2239.243246	63183.759703	60.149966
2238.535044	63014.313097	60.154970
2238.158550	62845.619518	60.159975
2237.045501	62664.010578	60.164980
2236.530557	62484.929788	60.169985
2235.626624	62308.331035	60.174990
2234.914215	62137.810251	60.179994
2234.461739	61955.780434	60.184999
2233.472190	61789.181580	60.190004
2233.107404	61619.617026	60.195009
2232.877592	61445.129046	60.200014
2231.947505	61264.546043	60.205018
2231.629956	61086.412722	60.210023
2230.687294	60911.178569	60.215028
2230.084933	60716.164704	60.220033
2229.184490	60549.328458	60.225038
2228.497490	60369.687304	60.230042
2227.910962	60187.499613	60.235047
2227.007829	60014.787237	60.240052
2226.714380	59837.583083	60.245057
2225.844662	59664.773682	60.250062
2224.975180	59490.367374	60.255066
2224.494473	59314.388037	60.260071
2223.882245	59142.489045	60.265076
2223.172873	58963.744901	60.270081
2222.622091	58788.560288	60.275086
2221.940925	58620.101770	60.280090
2221.575045	58428.565442	60.285095
2220.723290	58244.815117	60.290100
2220.220585	58077.254257	60.295105
2219.349790	57900.543100	60.300110
2218.453088	57718.818075	60.305114
2218.161463	57547.000113	60.310119
2217.142456	57379.109699	60.315124
2216.679465	57190.067067	60.320129
2216.119142	57020.037322	60.325134
2215.239420	56847.546930	60.330138
2214.712467	56655.655747	60.335143
2213.643038	56490.003127	60.340148
2213.328899	56317.402672	60.345153
2213.067961	56144.637162	60.350158
2212.005436	55960.443004	60.355162
2211.445260	55783.370595	60.360167
2210.393332	55609.957089	60.365172
2209.833765	55431.976569	60.370177
2209.226811	55264.688858	60.375182
2208.768173	55094.050061	60.380186
2208.516615	54901.481656	60.385191
2207.374673	54734.172911	60.390196
2207.204913	54553.610701	60.395201
2206.194230	54387.603888	60.400206
2205.393981	54195.212255	60.405210
2205.075885	54012.438562	60.410215
2204.113868	53831.961721	60.415220
2203.732579	53658.270540	60.420225
2202.661895	53487.822992	60.425230
2202.192246	53297.125607	60.430234
2201.099646	53125.612274	60.435239
2200.530954	52954.052265	60.440244
2200.361324	52767.081386	60.445249
2199.656953	52596.590454	60.450254
2198.923290	52418.113343	60.455258
2198.292211	52238.843372	60.460263
2197.299069	52070.077000	60.465268
2196.843541	51886.704281	60.470273
2196.330027	51709.515479	60.475278
2195.358975	51532.869263	60.480282
2194.907532	51357.661020	60.485287
2194.481799	51179.666220	60.490292
2194.094279	51004.875234	60.495297
2192.682609	50827.492760	60.500302
2192.092373	50640.015908	60.505306
2191.309637	50459.284975	60.510311
2190.698338	50292.512190	60.515316
2190.400073	50098.474328	60.520321
2189.336429	49934.389828	60.525326
2188.665094	49764.455216	60.530330
2188.293984	49582.918084	60.535335
2187.795397	49419.340276	60.540340
2187.051613	49244.477510	60.545345
2186.408729	49056.396114	60.550350
2185.795456	48873.955590	60.555354
2185.359543	48682.767289	60.560359
2184.493193	48514.710336	60.565364
2183.862311	48335.900206	60.570369
2183.093321	48153.760680	60.575374
2182.098575	47970.801594	60.580378
2181.762220	47794.623182	60.585383
2180.688329	47620.005957	60.590388
2180.174050	47445.972279	60.595393
2179.577302	47267.227648	60.600398
2178.499088	47085.477167	60.605402
2178.178326	46910.630458	60.610407
2177.364600	46755.189988	60.615412
2176.957872	46565.348463	60.620417
2176.081456	46402.048288	60.625422
2175.423180	46224.924488	60.630426
2175.169384	46052.112648	60.635431
2174.192294	45874.302841	60.640436
2173.723237	45697.881817	60.645441
2172.907086	45524.348376	60.650446
2172.390535	45350.702710	60.655450
2171.838436	45171.700339	60.660455
2170.862691	45004.364798	60.665460
2170.553069	44817.044368	60.670465
2169.437508	44643.393237	60.675470
2168.673196	44471.155585	60.680474
2168.414926	44295.180208	60.685479
2167.773341	44118.397711	60.690484
2167.220959	43933.007045	60.695489
2166.530327	43760.736280	60.700494
2165.864585	43588.159679	60.705498
2165.140473	43406.789778	60.710503
2164.195086	43238.429143	60.715508
2163.911407	43053.599787	60.720513
2163.252916	42880.659088	60.725518
2162.575402	42696.032017	60.730522
2161.722777	42529.896170	60.735527
2161.250793	42346.780265	60.740532
2160.543639	42158.463804	60.745537
2159.426256	41997.700282	60.750542
2158.906854	41822.869780	60.755546
2158.351978	41640.084433	60.760551
2157.649939	41470.848676	60.765556
2157.527187	41285.310760	60.770561
2156.571242	41113.102201	60.775566
2155.947760	40931.441995	60.780570
2155.314195	40751.976559	60.785575
2154.547966	40580.304508	60.790580
2153.830736	40401.091590	60.795585
2153.085314	40237.800304	60.800590
2152.268617	40050.374911	60.805594
2152.025534	39872.655842	60.810599
2150.934540	39704.449387	60.815604
2150.718198	39522.368059	60.820609
2149.837983	39358.289272	60.825614
2149.170151	39179.070294	60.830618
2148.567330	38998.584557	60.835623
2147.608715	38823.060843	60.840628
2147.127285	38651.244484	60.845633
2146.323174	38482.837043	60.850638
2145.763460	38298.761974	60.855642
2145.665071	38114.362795	60.860647
2144.551998	37947.296420	60.865652
2144.092383	37769.249593	60.870657
2143.018685	37599.260848	60.875662
2142.640206	37416.703057	60.880666
2141.768470	37239.876348	60.885671
2140.942020	37064.244016	60.890676
2140.549849	36881.879122	60.895681
2139.643109	36712.620468	60.900686
2139.259057	36544.137270	60.905690
2138.491190	36372.629790	60.910695
2137.538463	36192.681593	60.915700
2137.112532	36007.271581	60.920705
2136.558998	35846.941513	60.925710
2135.907035	35670.605378	60.930714
2135.399624	35497.110439	60.935719
2134.505593	35329.226115	60.940724
2133.906681	35153.542911	60.945729
2133.225088	34972.894692	60.950734
2132.615521	34810.873405	60.955738
2131.815097	34625.204658	60.960743
2131.106930	34461.784778	60.965748
2130.632159	34275.639970	60.970753
2129.718598	34102.508437	60.975758
2128.999600	33936.826032	60.980762
2128.558857	33772.670398	60.985767
2127.820574	33599.453084	60.990772
2127.409766	33415.498073	60.995777
2126.421909	33259.637640	61.000782
2125.685747	33076.999072	61.005786
2125.233600	32915.189364	61.010791
2124.395858	32750.629604	61.015796
2123.566180	32567.006476	61.020801
2123.263138	32408.603973	61.025806
2122.608632	32226.277886	61.030810
2122.074476	32052.282733	61.035815
2121.232393	31886.861601	61.040820
2120.833654	31717.065921	61.045825
2119.733910	31553.858541	61.050830
2119.166041	31371.771502	61.055834
2118.572556	31192.362465	61.060839
2117.564722	31025.765950	61.065844
2117.182967	30854.560742	61.070849
2116.259892	30695.393016	61.075854
2115.710903	30528.968909	61.080858
2115.116170	30362.075011	61.085863
2113.966792	30188.170357	61.090868
2113.428430	30016.878673	61.095873
2113.244281	29864.684790	61.100878
2112.298623	29695.546640	61.105882
2112.119997	29527.512980	61.110887
2110.867695	29360.066925	61.115892
2110.400288	29197.180848	61.120897
2109.773660	29030.060742	61.125902
2109.016221	28855.536193	61.130906
2108.096213	28693.693843	61.135911
2107.234774	28536.580132	61.140916
2107.071700	28368.674448	61.145921
2105.984731	28208.744978	61.150926
2105.244279	28044.036985	61.155930
2104.834607	27885.298656	61.160935
2103.928379	27738.142821	61.165940
2103.577735	27579.693535	61.170945
2102.820572	27417.278073	61.175950
2102.058257	27252.708768	61.180954
2101.695656	27091.826310	61.185959
2100.771422	26933.365374	61.190964
2100.490564	26768.254660	61.195969
2099.657394	26615.746382	61.200974
2098.345525	26454.034426	61.205978
2098.102700	26291.117453	61.210983
2097.329323	26130.898958	61.215988
2096.487440	25977.921861	61.220993
2095.848971	25823.260143	61.225998
2094.990003	25672.515059	61.231002
2094.537830	25517.807769	61.236007
2093.684017	25372.349012	61.241012
2093.167392	25216.876149	61.246017
2092.367845	25071.443104	61.251022
2091.555063	24925.515157	61.256026
2090.741493	24774.558091	61.261031
2089.943421	24633.146940	61.266036
2089.663100	24484.716448	61.271041
2088.355444	24347.316731	61.276046
2087.748787	24200.591944	61.281050
2087.028873	24073.477206	61.286055
2085.965784	23944.310260	61.291060
2085.181406	23803.379686	61.296065
2084.250429	23690.223583	61.301070
2083.636629	23572.419709	61.306074
2082.547785	23453.044061	61.311079
2081.599951	23338.050856	61.316084
2080.489470	23234.043882	61.321089
2079.288336	23148.430246	61.326094
2078.203119	23050.400478	61.331098
2077.279224	22970.818539	61.336103
2075.857155	22902.325948	61.341108
2075.053488	22833.077760	61.346113
2074.322540	22765.775827	61.351118
2073.458385	22716.561185	61.356122
2073.069710	22648.286312	61.361127
2072.318036	22581.260873	61.366132
2071.935589	22531.584242	61.371137
2070.938324	22472.300962	61.376142
2070.442446	22407.637677	61.381146
2069.618218	22352.776060	61.386151
2069.002332	22304.894066	61.391156
2068.437538	22241.266518	61.396161
2067.643363	22180.753488	61.401166
2067.119611	22136.543240	61.406170
2067.034531	22058.626753	61.411175
2066.253746	22008.981025	61.416180
2065.778302	21940.167897	61.421185
2065.009214	21885.890557	61.426190
2064.456348	21810.446709	61.431194
2064.045754	21757.364408	61.436199
2063.304083	21687.097590	61.441204
2062.866597	21621.827391	61.446209
2062.126073	21552.948268	61.451214
2061.334989	21492.794276	61.456218
2060.779214	21414.931184	61.461223
2060.104004	21366.068189	61.466228
2059.544449	21289.582520	61.471233
2058.638205	21234.533321	61.476238
2057.766294	21167.956174	61.481242
2057.755251	21104.305346	61.486247
2056.986106	21049.565858	61.491252
2056.667287	20986.388334	61.496257
2055.839735	20917.392374	61.501262
2055.281135	20850.698162	61.506266
2054.706930	20772.776828	61.511271
2054.050316	20709.487827	61.516276
2053.688669	20628.381687	61.521281
2052.721111	20576.615519	61.526286
2051.785832	20502.732008	61.531290
2051.163246	20427.142825	61.536295
2050.384442	20357.828549	61.541300
2049.698249	20287.077590	61.546305
2049.015671	20230.162008	61.551310
2048.238530	20167.688167	61.556314
2047.729006	20102.042544	61.561319
2047.033609	20035.918259	61.566324
2046.805809	19973.748024	61.571329
2045.789245	19913.485081	61.576334
2045.233854	19847.603852	61.581338
2045.031307	19765.235861	61.586343
2043.796484	19716.225636	61.591348
2043.363844	19643.096157	61.596353
2042.492583	19580.674337	61.601358
2041.919482	19506.775159	61.606362
2041.567419	19449.815888	61.611367
2040.578987	19393.073866	61.616372
2039.973453	19319.133356	61.621377
2039.816274	19252.732370	61.626382
2038.921408	19194.354686	61.631386
2038.729875	19114.622376	61.636391
2037.830133	19041.850490	61.641396
2037.134486	18979.301369	61.646401
2036.320353	18905.735778	61.651406
2035.554066	18835.652625	61.656410
2034.925949	18765.453918	61.661415
2034.212633	18704.171399	61.666420
2033.804819	18646.407643	61.671425
2033.101122	18565.577261	61.676430
2032.221282	18497.581535	61.681434
2031.765420	18432.303074	61.686439
2030.749786	18372.680241	61.691444
2030.490742	18288.158926	61.696449
2029.709232	18226.873323	61.701454
2028.814894	18158.463394	61.706458
2028.142755	18100.222219	61.711463
2027.614155	18028.115711	61.716468
2026.711097	17964.844985	61.721473
2026.175565	17904.494144	61.726478
2025.489808	17845.115821	61.731482
2025.109273	17776.573935	61.736487
2024.132032	17716.766764	61.741492
2023.675794	17645.253633	61.746497
2022.979852	17583.271031	61.751502
2022.263073	17521.109837	61.756506
2021.865243	17442.675898	61.761511
2020.785495	17383.806679	61.766516
2020.600459	17318.562542	61.771521
2019.959576	17241.670733	61.776526
2018.886115	17187.621241	61.781530
2018.555233	17125.443608	61.786535
2017.747593	17052.182372	61.791540
2017.275904	17001.004965	61.796545
2016.359072	16938.791232	61.801550
2015.903425	16874.521752	61.806554
2015.404874	16808.641224	61.811559
2014.455980	16740.860517	61.816564
2014.111020	16669.524461	61.821569
2013.636987	16597.015374	61.826574
2012.619526	16527.926350	61.831578
2011.827710	16456.897216	61.836583
2010.958721	16396.964119	61.841588
2010.437435	16326.337820	61.846593
2009.770687	16268.171951	61.851598
2009.345595	16206.203784	61.856602
2008.437800	16139.101944	61.861607
2007.607204	16083.912373	61.866612
2007.154029	16015.323521	61.871617
2006.248534	15953.475633	61.876622
2005.537595	15890.703056	61.881626
2005.179306	15840.224225	61.886631
2004.647273	15767.243630	61.891636
2003.955961	15702.761303	61.896641
2002.997551	15653.886139	61.901646
2002.256077	15573.906813	61.906650
2001.770786	15506.074145	61.911655
2001.032878	15460.545702	61.916660
2000.515323	15391.801242	61.921665
1999.950686	15321.561036	61.926670
1999.334621	15260.143259	61.931674
1998.777184	15197.677676	61.936679
1997.856929	15146.454603	61.941684
1997.848197	15077.470377	61.946689
1996.829656	15020.168713	61.951694
1995.842430	14926.638434	61.956698
1995.515804	14867.446717	61.961703
1994.611947	14815.691589	61.966708
1993.921376	14745.191466	61.971713
1993.375903	14688.912486	61.976718
1992.737590	14622.035667	61.981722
1992.503787	14550.451673	61.986727
1991.662552	14494.731562	61.991732
1990.742586	14418.871546	61.996737
1990.117410	14358.877921	62.001742
1989.438728	14294.678200	62.006746
1988.894775	14232.391786	62.011751
1987.817240	14179.302451	62.016756
1987.332319	14110.994981	62.021761
1986.669366	14046.639914	62.026766
1985.626301	13985.547369	62.031770
1985.342611	13913.631074	62.036775
1984.572005	13877.951155	62.041780
1984.153964	13803.565635	62.046785
1983.200326	13733.366837	62.051790
1982.762087	13679.011281	62.056794
1982.000431	13610.496947	62.061799
1981.349325	13555.623695	62.066804
1980.885458	13489.689957	62.071809
1980.071857	13420.847355	62.076814
1979.552915	13364.920315	62.081818
1978.878499	13306.791573	62.086823
1977.841943	13250.248716	62.091828
1977.174749	13186.171492	62.096833
1976.662692	13131.033757	62.101838
1975.977077	13076.826937	62.106842
1975.558390	13014.047004	62.111847
1974.586340	12955.659873	62.116852
1974.173905	12890.883348	62.121857
1973.632289	12828.891118	62.126862
1972.832831	12772.923779	62.131866
1972.395645	12694.621940	62.136871
1971.647343	12638.956309	62.141876
1971.256493	12565.765782	62.146881
1970.159652	12502.317145	62.151886
1969.296568	12442.580904	62.156890
1969.194021	12386.301769	62.161895
1968.313013	12325.724297	62.166900
1967.590164	12252.070133	62.171905
1967.266736	12190.017076	62.176910
1965.990598	12133.150472	62.181914
1965.725318	12059.554616	62.186919
1964.837671	12011.562994	62.191924
1964.393017	11943.996945	62.196929
1963.615895	11889.127328	62.201934
1962.623387	11823.287887	62.206938
1962.239813	11759.032793	62.211943
1962.142087	11696.081506	62.216948
1961.462143	11625.310969	62.221953
1960.513964	11566.390027	62.226958
1959.727930	11505.767227	62.231962
1959.163900	11428.666371	62.236967
1958.142437	11371.275958	62.241972
1957.632504	11314.906866	62.246977
1957.116250	11247.580366	62.251982
1956.357961	11180.423566	62.256986
1955.924808	11125.350430	62.261991
1955.336494	11065.778597	62.266996
1954.099695	10997.403370	62.272001
1953.564910	10938.884195	62.277006
1952.927091	10883.391923	62.282010
1952.505925	10815.777675	62.287015
1951.768811	10760.763193	62.292020
1950.943314	10694.671773	62.297025
1950.117393	10629.852989	62.302030
1949.510443	10575.532971	62.307034
1948.942591	10522.339559	62.312039
1948.321368	10454.805632	62.317044
1947.759353	10393.398644	62.322049
1947.067608	10336.270704	62.327054
1946.399033	10260.221657	62.332058
1945.939105	10192.875934	62.337063
1945.235673	10141.646692	62.342068
1944.604834	10079.998644	62.347073
1943.872239	10016.340117	62.352078
1942.788860	9957.117536	62.357082
1942.392907	9894.290134	62.362087
1941.589000	9842.872334	62.367092
1941.155974	9775.240972	62.372097
1940.440392	9716.325066	62.377102
1939.949315	9665.720550	62.382106
1939.317693	9590.364889	62.387111
1938.559828	9544.505704	62.392116
1938.128182	9481.645457	62.397121
1937.303177	9409.343082	62.402126
1936.740897	9349.658727	62.407130
1936.119582	9271.155150	62.412135
1935.340818	9222.145303	62.417140
1934.553725	9169.585554	62.422145
1933.519312	9094.157080	62.427150
1932.927780	9031.530406	62.432154
1932.539765	8966.681242	62.437159
1931.445429	8918.604107	62.442164
1931.010898	8865.752388	62.447169
1930.445144	8803.285883	62.452174
1929.294658	8756.935255	62.457178
1928.895339	8707.364325	62.462183
1928.093513	8646.076715	62.467188
1927.934429	8584.060541	62.472193
1927.375987	8531.690786	62.477198
1926.609085	8473.499507	62.482202
1926.182163	8392.968246	62.487207
1925.425380	8343.100267	62.492212
1924.526493	8275.227367	62.497217
1923.574612	8214.241461	62.502222
1923.255925	8163.231657	62.507226
1922.777370	8104.955019	62.512231
1921.929481	8045.701447	62.517236
1921.115846	7976.863411	62.522241
1920.754676	7921.170553	62.527246
1919.958482	7880.046307	62.532250
1919.381153	7802.218730	62.537255
1918.785992	7748.303103	62.542260
1918.173598	7692.505041	62.547265
1917.711678	7626.473576	62.552270
1916.710204	7551.739100	62.557274
1916.416877	7489.707365	62.562279
1915.325390	7441.252356	62.567284
1914.877533	7369.482941	62.572289
1913.957734	7317.234376	62.577294
1913.275337	7259.907665	62.582298
1912.795773	7188.910111	62.587303
1912.078390	7133.589123	62.592308
1911.461166	7065.251060	62.597313
1910.730276	7016.096516	62.602318
1910.094384	6965.477995	62.607322
1909.893030	6895.384258	62.612327
1908.705291	6845.409079	62.617332
1908.127737	6765.513965	62.622337
1907.284944	6720.461030	62.627342
1906.729724	6652.150521	62.632346
1906.057341	6587.798969	62.637351
1905.364851	6538.364622	62.642356
1904.619426	6471.472631	62.647361
1904.216519	6415.639798	62.652366
1903.537538	6358.195344	62.657370
1903.200257	6290.647785	62.662375
1901.876228	6230.782918	62.667380
1901.872936	6166.679557	62.672385
1900.864193	6118.698471	62.677390
1899.818202	6050.653220	62.682394
1898.991126	5994.308781	62.687399
1898.448955	5949.828072	62.692404
1897.946770	5892.041855	62.697409
1897.172766	5841.147009	62.702414
1896.750640	5775.903454	62.707418
1895.813981	5730.112813	62.712423
1895.271403	5680.047831	62.717428
1895.059673	5612.031482	62.722433
1894.353902	5556.685359	62.727438
1893.553791	5506.814077	62.732442
1893.173944	5428.536943	62.737447
1892.073254	5375.039896	62.742452
1891.504651	5319.646858	62.747457
1890.881495	5259.829254	62.752462
1890.138298	5195.289935	62.757466
1889.525605	5151.974362	62.762471
1888.566183	5090.368381	62.767476
1888.116119	5038.264673	62.772481
1887.552838	4974.213578	62.777486
1886.507187	4933.183665	62.782490
1885.988604	4860.509322	62.787495
1885.472567	4810.724645	62.792500
1884.728447	4758.828717	62.797505
1884.028747	4697.479698	62.802510
1883.146922	4640.897530	62.807514
1882.879797	4582.831471	62.812519
1882.031459	4538.964386	62.817524
1881.470498	4481.390197	62.822529
1880.956353	4426.279743	62.827534
1880.183107	4372.527725	62.832538
1879.560496	4323.786110	62.837543
1878.685631	4261.058145	62.842548
1878.341554	4207.025654	62.847553
1877.602632	4162.242451	62.852558
1876.823505	4096.284591	62.857562
1876.276331	4026.562991	62.862567
1875.409928	3983.389725	62.867572
1875.003854	3917.573760	62.872577
1874.505416	3876.022225	62.877582
1873.438285	3812.344832	62.882586
1873.301958	3757.642992	62.887591
1872.177814	3692.048511	62.892596
1871.646850	3641.956285	62.897601
1870.949420	3589.094939	62.902606
1870.260289	3539.213506	62.907610
1869.746736	3472.703674	62.912615
1868.658768	3431.949668	62.917620
1867.970541	3360.193731	62.922625
1867.635749	3320.747866	62.927630
1866.694501	3267.302593	62.932634
1865.868214	3209.464805	62.937639
1865.489306	3169.081590	62.942644
1865.017902	3099.685163	62.947649
1864.146007	3060.594190	62.952654
1863.794295	3003.887651	62.957658
1863.563780	2943.280586	62.962663
1862.260462	2881.253497	62.967668
1861.781972	2813.286129	62.972673
1860.775088	2762.339567	62.977678
1860.020302	2713.761513	62.982682
1859.672473	2661.762778	62.987687
1858.958427	2622.360085	62.992692
1858.530344	2557.637240	62.997697
1857.719964	2515.578416	63.002702
1857.098152	2457.088166	63.007706
1856.483091	2398.322655	63.012711
1855.552719	2349.042687	63.017716
1854.829942	2286.836058	63.022721
1854.342042	2229.438917	63.027726
1853.291921	2182.527658	63.032730
1852.837588	2127.757806	63.037735
1852.115699	2082.263841	63.042740
1851.654940	2032.262978	63.047745
1850.966987	1977.645123	63.052750
1849.758178	1924.964836	63.057754
1849.693183	1872.294747	63.062759
1848.749497	1826.472491	63.067764
1847.974488	1786.256927	63.072769
1847.437959	1741.641418	63.077774
1846.685199	1687.624768	63.082778
1846.348729	1637.748251	63.087783
1845.381821	1587.350644	63.092788
1844.712983	1535.535425	63.097793
1843.779077	1501.064277	63.102798
1842.881106	1449.465531	63.107802
1842.723608	1400.785196	63.112807
1841.965911	1373.565985	63.117812
1841.524657	1315.831496	63.122817
1840.987331	1274.330606	63.127822
1839.991417	1220.685477	63.132826
1839.545237	1179.752304	63.137831
1838.861840	1129.522593	63.142836
1838.262512	1070.058969	63.147841
1837.278008	1031.491248	63.152846
1836.511651	980.135057	63.157850
1836.188156	940.487253	63.162855
1835.469736	909.774380	63.167860
1834.982450	852.804419	63.172865
1834.124532	818.330718	63.177870
1833.523437	764.687667	63.182874
1832.861473	714.985852	63.187879
1832.108287	679.152280	63.192884
1831.647526	634.239562	63.197889
1830.722519	577.100490	63.202894
1829.603845	539.839812	63.207898
1829.236866	493.982241	63.212903
1828.573831	460.235383	63.217908
1827.823713	426.008851	63.222913
1827.066261	386.735816	63.227918
1826.183167	341.369105	63.232922
1825.805881	302.439627	63.237927
1825.315764	271.576747	63.242932
1824.296820	240.572404	63.247937
1823.513653	191.798358	63.252942
1822.608011	171.306764	63.257946
1822.186695	129.473778	63.262951
1821.270213	104.281685	63.267956
1820.214306	79.592729	63.272961
1819.491035	61.956476	63.277966
1818.685402	37.317736	63.282970
1818.114740	20.980312	63.287975
1817.161809	10.024023	63.292980
1816.472945	-0.037517	63.297985
1815.560988	-5.295123	63.302990
1813.317000	42.580723	63.307994
1811.866502	38.323214	63.312999
1811.271972	58.191834	63.318004
1811.377447	60.594035	63.323009
1811.388103	46.272582	63.328014
1810.818223	59.878611	63.333018
1811.036081	62.958376	63.338023
1810.386586	54.213562	63.343028
1809.692753	61.055486	63.348033
1808.275715	55.890678	63.353038
1807.127241	70.277695	63.358042
1806.767217	59.359683	63.363047
1806.128834	60.539644	63.368052
1805.922272	64.517827	63.373057
1805.805028	59.357924	63.378062
1804.694490	69.135968	63.383066
1804.133052	62.531205	63.388071
1803.594468	60.464266	63.393076
1802.758358	67.224712	63.398081
1801.751810	71.153318	63.403086
1801.274358	84.637464	63.408090
1801.112737	66.533572	63.413095
1799.916718	71.615013	63.418100
1799.056877	70.852719	63.423105
1798.812563	67.398692	63.428110
1797.775255	73.842598	63.433114
1797.079018	65.772231	63.438119
1796.517352	75.720156	63.443124
1796.535769	77.611077	63.448129
1795.316733	73.493423	63.453134
1795.052459	76.673404	63.458138
1794.625314	73.019760	63.463143
1793.253866	77.328002	63.468148
1792.268300	80.646177	63.473153
1792.432195	74.072881	63.478158
1792.019497	78.377104	63.483162
1791.329847	80.260622	63.488167
1790.077360	78.412702	63.493172
1789.211151	70.605860	63.498177
1789.406166	70.951765	63.503182
1788.406579	83.123275	63.508186
1787.523780	71.256987	63.513191
1786.454027	79.746552	63.518196
1786.582812	75.392792	63.523201
1786.361553	72.469671	63.528206
1784.681656	72.495171	63.533210
1784.039256	78.048503	63.538215
1783.298484	71.677217	63.543220
1783.548332	73.458848	63.548225
1782.512829	69.256866	63.553230
1781.414172	77.468758	63.558234
1781.141888	59.261033	63.563239
1780.541678	71.146770	63.568244
1779.961666	81.644797	63.573249
1779.114487	70.581804	63.578254
1778.423532	75.160442	63.583258
1778.017951	77.445112	63.588263
1777.048491	70.193970	63.593268
1776.579701	67.571924	63.598273
1776.040231	62.037545	63.603278
1775.161840	79.656895	63.608282
1774.637212	57.857660	63.613287
1774.306389	77.403742	63.618292
1773.460017	63.927981	63.623297
1773.006668	68.380579	63.628302
1771.622256	63.440835	63.633306
1770.799093	68.893567	63.638311
1770.656845	67.484334	63.643316
1770.462636	68.981682	63.648321
1769.053875	64.927289	63.653326
1768.083165	65.258053	63.658330
1767.777089	56.652672	63.663335
1767.453017	72.208139	63.668340
1766.620173	68.128516	63.673345
1766.284375	66.030958	63.678350
1765.172591	68.844079	63.683354
1764.857562	58.278465	63.688359
1764.138384	62.221366	63.693364
1763.737294	65.842528	63.698369
1763.263758	61.157088	63.703374
1762.240479	59.790005	63.708378
1761.198409	58.939974	63.713383
1760.340520	68.629024	63.718388
1759.848132	62.696103	63.723393
1759.743523	63.931649	63.728398
1759.087308	67.594905	63.733402
1758.348172	50.245055	63.738407
1757.342377	65.319023	63.743412
1756.881373	64.671592	63.748417
1756.460809	64.894490	63.753422
1755.506652	79.425705	63.758426
1755.569065	61.253138	63.763431
1753.670929	66.264758	63.768436
1753.040438	73.251175	63.773441
1752.551481	64.022004	63.778446
1751.856896	66.218537	63.783450
1752.060969	59.597869	63.788455
1750.627250	72.510081	63.793460
1750.042717	51.516711	63.798465
1749.821625	67.070009	63.803470
1749.043283	66.944468	63.808474
1748.703479	52.338069	63.813479
1747.869685	68.509049	63.818484
1747.018550	65.600816	63.823489
1746.010550	58.661731	63.828494
1745.145659	69.778985	63.833498
1744.900173	68.865524	63.838503
1744.417455	67.625478	63.843508
1743.804460	73.019610	63.848513
1743.427394	69.533059	63.853518
1742.503787	71.463205	63.858522
1742.120232	61.036206	63.863527
1740.761185	73.425651	63.868532
1739.882645	74.203816	63.873537
1739.512872	74.595263	63.878542
1738.600257	68.607664	63.883546
1738.519438	63.645401	63.888551
1737.833164	70.752637	63.893556
1737.357503	65.070944	63.898561
1737.270698	67.937324	63.903566
1736.155920	69.420035	63.908570
1735.026039	65.841744	63.913575
1733.990795	72.353149	63.918580
1733.423587	74.922105	63.923585
1733.311104	68.235018	63.928590
1732.484597	75.987403	63.933594
1732.337188	67.544474	63.938599
1731.728434	72.184180	63.943604
1730.352287	57.824373	63.948609
1729.617319	61.728790	63.953614
1728.606648	79.528422	63.958618
1728.255992	64.046988	63.963623
1727.555973	64.096664	63.968628
1727.197116	65.393091	63.973633
1727.000667	62.920184	63.978638
1726.449803	67.484465	63.983642
1725.820380	66.201494	63.988647
1724.283495	62.495471	63.993652
1723.606458	65.651128	63.998657
1723.334082	63.914073	64.003662
1722.608084	61.738152	64.008666
1722.419128	70.288105	64.013671
1721.629162	68.743638	64.018676
1720.553460	68.365724	64.023681
1719.390868	62.354763	64.028686
1718.652441	69.722588	64.033690
1718.387651	57.748727	64.038695
1717.592033	81.577353	64.043700
1717.052675	65.655977	64.048705
1716.615721	67.907792	64.053710
1715.820963	79.887518	64.058714
1716.141493	64.472943	64.063719
1715.471738	70.943649	64.068724
1714.551727	63.976410	64.073729
1713.513841	66.642201	64.078734
1712.818345	71.752986	64.083738
1712.442696	65.003626	64.088743
1711.266186	67.757666	64.093748
1710.332997	66.511907	64.098753
1709.917545	62.927385	64.103758
1709.303519	67.626276	64.108762
1708.858245	68.854433	64.113767
1708.575215	70.257087	64.118772
1707.740784	66.628729	64.123777
1706.555262	64.461146	64.128782
1705.608248	70.542247	64.133786
1705.273648	62.504357	64.138791
1704.341439	72.255687	64.143796
1703.711198	68.637474	64.148801
1703.418822	71.791963	64.153806
1702.862847	72.436908	64.158810
1702.840321	66.771556	64.163815
1702.524724	72.189418	64.168820
1701.104729	71.904043	64.173825
1700.344300	66.166667	64.178830
1699.423507	76.064416	64.183834
1698.844089	66.286676	64.188839
1698.005143	75.799278	64.193844
1697.219791	71.199646	64.198849
1696.601613	59.291380	64.203854
1695.634125	80.345170	64.208858
1695.255260	69.843318	64.213863
1695.056978	75.184203	64.218868
1694.562400	66.086822	64.223873
1694.252734	69.379670	64.228878
1693.537899	72.880371	64.233882
1692.558257	66.417755	64.238887
1691.547746	76.301372	64.243892
1691.137516	69.858694	64.248897
1690.441140	69.018435	64.253902
1689.230558	73.365826	64.258906
1688.825679	70.006700	64.263911
1687.907180	73.437254	64.268916
1687.798079	77.210736	64.273921
1687.354049	70.445434	64.278926
1686.640387	69.737226	64.283930
1685.975140	62.136622	64.288935
1684.592412	75.824479	64.293940
1683.795097	65.865321	64.298945
1683.779056	62.800812	64.303950
1682.976961	79.964950	64.308954
1682.797930	64.238658	64.313959
1682.340581	76.436018	64.318964
1680.918310	68.108867	64.323969
1680.491651	61.143701	64.328974
1679.657783	78.032197	64.333978
1679.067130	70.497010	64.338983
1678.785721	70.155367	64.343988
1677.838432	72.589171	64.348993
1676.939407	62.149453	64.353998
1676.103512	62.268033	64.359002
1675.873497	59.213860	64.364007
1675.392616	72.320090	64.369012
1674.837834	71.326461	64.374017
1674.081582	55.128918	64.379022
1673.214123	74.530002	64.384026
1672.951358	54.031158	64.389031
1672.098403	68.234080	64.394036
1670.833027	73.244592	64.399041
1670.069041	63.209188	64.404046
1669.514348	62.734344	64.409050
1668.829194	69.893452	64.414055
1668.261219	65.328686	64.419060
1667.954469	68.017123	64.424065
1667.784257	63.181025	64.429070
1667.014992	68.000773	64.434074
1666.191618	69.110808	64.439079
1665.168274	62.084314	64.444084
1664.629779	60.072584	64.449089
1664.585222	69.788573	64.454094
1662.971442	65.618581	64.459098
1662.589719	55.235469	64.464103
1661.764996	71.469676	64.469108
1661.201549	65.056076	64.474113
1661.225756	60.629049	64.479118
1659.803678	77.797057	64.484122
1658.962123	65.531637	64.489127
1658.337103	67.352881	64.494132
1657.788512	67.017414	64.499137
1657.322903	60.802733	64.504142
1656.814318	78.100013	64.509146
1656.703353	69.209776	64.514151
1655.478988	69.421608	64.519156
1654.295636	64.016349	64.524161
1654.087706	69.781373	64.529166
1653.097211	73.352679	64.534170
1653.215238	65.867347	64.539175
1652.255293	75.941631	64.544180
1651.105837	64.549840	64.549185
1650.880025	61.400389	64.554190
1650.176901	76.054164	64.559194
1649.548285	65.997262	64.564199
1648.511587	55.174172	64.569204
1647.557925	62.606160	64.574209
1647.337674	58.490769	64.579214
1646.399529	68.503241	64.584218
1645.969699	62.778022	64.589223
1645.658341	58.861600	64.594228
1645.278823	72.532025	64.599233
1644.454673	65.696237	64.604238
1643.672435	71.740143	64.609242
1643.107745	66.078922	64.614247
1642.005329	64.248239	64.619252
1641.174822	73.283290	64.624257
1640.755491	59.124771	64.629262
1640.160324	71.719322	64.634266
1639.602223	57.338432	64.639271
1638.919984	60.302553	64.644276
1638.703686	64.499898	64.649281
1637.899153	51.594709	64.654286
1636.807304	71.069284	64.659290
1636.625534	64.554060	64.664295
1635.240620	67.388544	64.669300
1634.550737	65.823476	64.674305
1633.714314	64.021501	64.679310
1633.107074	71.359043	64.684314
1633.201036	56.850916	64.689319
1632.623060	58.346160	64.694324
1632.333162	64.179394	64.699329
1630.925072	68.665413	64.704334
1630.166249	63.558565	64.709338
1629.777152	60.761471	64.714343
1629.299764	54.531325	64.719348
1628.068264	59.709928	64.724353
1627.297030	62.877417	64.729358
1626.736517	60.301513	64.734362
1626.629957	60.916078	64.739367
1625.935775	57.238665	64.744372
1625.209854	60.679641	64.749377
1624.391590	61.248004	64.754382
1623.516910	68.459305	64.759386
1623.360568	63.797620	64.764391
1622.756051	67.698687	64.769396
1621.410808	58.435285	64.774401
1620.508584	57.741284	64.779406
1619.739106	71.347507	64.784410
1619.719083	60.050690	64.789415
1619.319784	60.959333	64.794420
1618.913247	60.421541	64.799425
1617.957248	61.767117	64.804430
1616.356910	61.016873	64.809434
1616.077166	62.688660	64.814439
1615.406632	64.853021	64.819444
1614.900536	62.465587	64.824449
1614.728241	68.332177	64.829454
1614.196804	63.372130	64.834458
1613.454698	53.560351	64.839463
1612.606754	63.818685	64.844468
1611.752763	54.070411	64.849473
1611.526116	60.354047	64.854478
1610.361367	75.748188	64.859482
1609.464646	54.410253	64.864487
1609.042603	71.201787	64.869492
1608.045193	66.489227	64.874497
1608.321515	63.687343	64.879502
1607.329194	61.203698	64.884506
1606.583455	69.367460	64.889511
1605.447762	73.699835	64.894516
1605.014282	63.764908	64.899521
1604.907932	59.122092	64.904526
1604.184095	73.846967	64.909530
1603.281456	52.224562	64.914535
1602.474089	64.411293	64.919540
1601.850062	63.868635	64.924545
1601.672073	58.524447	64.929550
1600.373130	65.079363	64.934554
1599.745259	70.996257	64.939559
1598.580110	71.006327	64.944564
1598.679228	68.516435	64.949569
1598.277162	54.467151	64.954574
1597.763880	74.855875	64.959578
1596.815998	65.362205	64.964583
1596.027160	72.496801	64.969588
1595.485760	65.980373	64.974593
1595.025897	57.583958	64.979598
1593.546353	68.488247	64.984602
1593.238373	52.184835	64.989607
1592.441715	74.922414	64.994612
1591.942094	58.504368	64.999617
1591.641984	63.798354	65.004622
1590.568580	63.316055	65.009626
1590.143025	56.960993	65.014631
1589.146693	66.957492	65.019636
1588.665537	64.167147	65.024641
1588.528193	64.919063	65.029646
1587.349674	56.777171	65.034650
1586.709799	64.212938	65.039655
1585.952613	61.956861	65.044660
1585.614094	62.778585	65.049665
1585.102504	63.913223	65.054670
1583.391873	67.613157	65.059674
1583.187518	60.049746	65.064679
1582.608730	63.088904	65.069684
1581.969149	60.801529	65.074689
1581.820700	67.839113	65.079694
1581.148149	63.377715	65.084698
1580.213915	59.445153	65.089703
1579.321309	71.270137	65.094708
1578.796367	64.120344	65.099713
1578.461323	63.427703	65.104718
1577.374353	66.896095	65.109722
1576.779343	60.416576	65.114727
1576.172912	65.040170	65.119732
1575.976216	73.815270	65.124737
1574.895874	69.752963	65.129742
1573.832566	67.821482	65.134746
1573.662440	64.272123	65.139751
1573.051180	69.405821	65.144756
1572.155726	64.514659	65.149761
1571.474102	58.356397	65.154766
1570.260714	74.718601	65.159770
1570.036382	63.941508	65.164775
1569.585912	60.059817	65.169780
1569.074654	69.468341	65.174785
1568.720975	63.533929	65.179790
1567.773777	62.615289	65.184794
1567.155378	53.782044	65.189799
1566.630732	62.388478	65.194804
1565.673804	66.925843	65.199809
1564.923799	58.927181	65.204814
1564.340982	69.427244	65.209818
1563.833611	66.149079	65.214823
1562.299903	60.950917	65.219828
1561.611192	62.501616	65.224833
1561.166178	71.492780	65.229838
1560.636923	61.054287	65.234842
1560.758015	59.983258	65.239847
1560.263917	64.538546	65.244852
1559.681763	57.929263	65.249857
1558.742310	62.123245	65.254862
1557.735728	69.371290	65.259866
1557.145550	57.561126	65.264871
1555.955659	57.745451	65.269876
1555.058659	60.327416	65.274881
1554.725766	58.324043	65.279886
1554.254069	79.234422	65.284890
1554.611167	59.993244	65.289895
1553.228866	71.268441	65.294900
1552.307215	65.309163	65.299905
1551.965839	57.553073	65.304910
1551.297532	60.532346	65.309914
1550.392507	59.805699	65.314919
1549.212928	71.756710	65.319924
1548.865912	63.250914	65.324929
1548.427856	67.344732	65.329934
1547.653872	75.963987	65.334938
1547.528247	57.780340	65.339943
1546.595508	69.297906	65.344948
1545.879843	67.131434	65.349953
1545.519699	63.016207	65.354958
1544.234401	61.476389	65.359962
1543.418864	70.422353	65.364967
1542.679709	63.539987	65.369972
1542.483265	70.763386	65.374977
1542.375133	66.412581	65.379982
1541.566228	74.633702	65.384986
1541.002633	71.045944	65.389991
1539.859785	65.930762	65.394996
1539.205044	67.056617	65.400001
1538.475098	61.147308	65.405006
1537.086531	72.850844	65.410010
1536.760751	66.339593	65.415015
1536.131997	67.201133	65.420020
1535.980195	67.602126	65.425025
1535.751570	67.758292	65.430030
1534.988008	72.480978	65.435034
1534.180648	66.016288	65.440039
1533.580943	67.552852	65.445044
1532.861709	70.895023	65.450049
1531.727781	66.636256	65.455054
1530.804775	71.012131	65.460058
1530.284819	64.653157	65.465063
1529.963638	64.227968	65.470068
1529.760221	68.393311	65.475073
1528.949251	70.546894	65.480078
1527.794051	73.750193	65.485082
1527.454729	68.559375	65.490087
1526.621515	75.898151	65.495092
1526.054560	68.187366	65.500097
1525.201158	69.524557	65.505102
1524.477140	80.179527	65.510106
1524.019165	66.180138	65.515111
1523.638001	61.740262	65.520116
1522.771312	60.898729	65.525121
1522.174960	73.558133	65.530126
1521.352635	71.891144	65.535130
1521.249668	62.841970	65.540135
1520.275897	62.971470	65.545140
1518.925600	67.213404	65.550145
1518.727736	65.470842	65.555150
1518.173519	68.286921	65.560154
1517.597530	69.354537	65.565159
1516.704385	71.432876	65.570164
1516.026034	63.831258	65.575169
1515.981384	65.684885	65.580174
1514.601983	63.218633	65.585178
1513.854117	56.742925	65.590183
1513.363670	63.461128	65.595188
1512.534504	66.035482	65.600193
1512.201462	67.513907	65.605198
1511.817255	67.112927	65.610202
1511.119100	62.881115	65.615207
1510.211777	65.412698	65.620212
1509.594423	66.551541	65.625217
1508.922109	62.883303	65.630222
1507.771297	67.754258	65.635226
1507.249701	64.011609	65.640231
1506.962786	62.614346	65.645236
1506.346554	71.378842	65.650241
1505.535392	60.384371	65.655246
1504.635222	63.919296	65.660250
1504.076302	60.299270	65.665255
1503.524052	61.464037	65.670260
1503.184854	61.757621	65.675265
1502.828503	62.610573	65.680270
1501.421250	68.427415	65.685274
1500.940044	56.868027	65.690279
1500.478604	57.542144	65.695284
1499.448408	66.471765	65.700289
1498.748383	60.204493	65.705294
1498.017905	69.069142	65.710298
1497.488412	63.082262	65.715303
1496.957630	62.772383	65.720308
1496.318889	63.531444	65.725313
1495.768730	60.955504	65.730318
1495.143551	65.984199	65.735322
1494.685584	56.464766	65.740327
1493.844828	66.222111	65.745332
1492.850228	72.151572	65.750337
1492.691200	62.483710	65.755342
1491.519479	63.264394	65.760346
1490.475855	54.183371	65.765351
1490.106544	56.113820	65.770356
1489.710211	54.953135	65.775361
1489.457580	58.724191	65.780366
1488.570451	73.049269	65.785370
1487.674702	59.507381	65.790375
1486.704431	60.271823	65.795380
1486.342858	69.721220	65.800385
1486.101749	56.665060	65.805390
1484.852342	63.598490	65.810394
1484.137055	59.481369	65.815399
1483.390451	60.643911	65.820404
1483.111408	66.620502	65.825409
1483.038200	52.839102	65.830414
1481.712987	67.378868	65.835418
1481.337377	60.282640	65.840423
1480.980278	67.935252	65.845428
1479.701856	54.400572	65.850433
1479.056589	55.865542	65.855438
1477.888699	70.861262	65.860442
1477.684987	53.260881	65.865447
1477.464258	68.266918	65.870452
1476.744524	70.945313	65.875457
1475.903338	50.510078	65.880462
1475.355875	68.157286	65.885466
1474.691335	67.846592	65.890471
1473.619725	62.291211	65.895476
1472.731581	60.320900	65.900481
1472.559987	63.525592	65.905486
1471.952376	64.420055	65.910490
1471.448606	63.640707	65.915495
1470.599698	66.738584	65.920500
1469.933584	70.706237	65.925505
1469.615339	62.322038	65.930510
1468.631619	58.230237	65.935514
1467.662174	62.285517	65.940519
1467.023677	63.500266	65.945524
1466.192950	63.275907	65.950529
1466.033705	61.426292	65.955534
1465.184090	65.024156	65.960538
1464.079861	49.473353	65.965543
1463.779178	58.528307	65.970548
1463.059633	59.787476	65.975553
1463.001922	53.550597	65.980558
1462.370200	63.134383	65.985562
1461.631909	62.422269	65.990567
1460.352312	63.341532	65.995572
1460.097640	59.745701	66.000577
1459.888024	59.193985	66.005582
1458.710666	62.113838	66.010586
1458.193388	65.132207	66.015591
1457.467295	67.054710	66.020596
1456.088481	59.001489	66.025601
1455.700798	59.141942	66.030606
1455.121613	65.445343	66.035610
1454.834094	63.884186	66.040615
1454.399185	54.976087	66.045620
1453.456578	60.064697	66.050625
1452.751278	59.043003	66.055630
1451.924197	69.545631	66.060634
1451.742223	60.614676	66.065639
1450.605559	61.506496	66.070644
1449.555048	63.950474	66.075649
1449.369941	51.090422	66.080654
1448.723874	59.561630	66.085658
1448.476546	50.450266	66.090663
1447.697788	60.319184	66.095668
1446.816428	64.442470	66.100673
1446.591765	61.299168	66.105678
1444.824820	62.997608	66.110682
1444.451624	59.836914	66.115687
1443.769785	61.780772	66.120692
1443.372504	63.496485	66.125697
1443.168903	56.349277	66.130702
1442.571411	62.567282	66.135706
1442.132153	62.786894	66.140711
1441.182177	54.365920	66.145716
1440.113642	61.284813	66.150721
1439.252434	57.268166	66.155726
1438.403318	59.738483	66.160730
1437.929854	54.146401	66.165735
1437.738433	61.417880	66.170740
1437.276722	66.540448	66.175745
1436.483375	73.190116	66.180750
1435.436565	65.847351	66.185754
1435.044917	59.684046	66.190759
1434.066254	67.522176	66.195764
1433.222229	58.606567	66.200769
1432.839094	64.353709	66.205774
1431.908146	68.117467	66.210778
1431.942714	58.478770	66.215783
1430.923024	59.695769	66.220788
1429.881517	63.600095	66.225793
1429.422011	59.223151	66.230798
1429.087011	64.588921	66.235802
1428.861550	60.838647	66.240807
1427.801768	70.758549	66.245812
1426.862179	61.006610	66.250817
1426.499406	61.346527	66.255822
1425.527511	68.321029	66.260826
1424.893202	55.423569	66.265831
1424.625518	66.682500	66.270836
1424.177747	60.668460	66.275841
1423.327448	60.111350	66.280846
1422.073775	63.204190	66.285850
1421.859134	67.254631	66.290855
1420.964279	64.796569	66.295860
1419.929529	69.735842	66.300865
1419.489200	57.428845	66.305870
1418.783235	58.297953	66.310874
1418.435324	73.965998	66.315879
1418.233312	58.889953	66.320884
1417.005404	63.308016	66.325889
1416.480561	50.126671	66.330894
1415.801140	54.813930	66.335898
1415.207222	58.273398	66.340903
1414.255183	68.756471	66.345908
1413.311050	69.128872	66.350913
1413.163422	57.208998	66.355918
1412.610780	64.474816	66.360922
1411.975340	60.201530	66.365927
1411.187124	64.253254	66.370932
1410.314437	66.124957	66.375937
1409.981872	62.292365	66.380942
1408.960040	63.279487	66.385946
1408.101738	58.872899	66.390951
1407.276649	64.278722	66.395956
1407.019755	62.958697	66.400961
1406.632093	62.036334	66.405966
1406.130942	66.947564	66.410970
1405.669299	60.349132	66.415975
1404.700389	56.822683	66.420980
1403.886447	59.626450	66.425985
1403.389039	63.838525	66.430990
1402.244430	64.974470	66.435994
1401.769944	64.838581	66.440999
1401.035928	59.997519	66.446004
1400.585680	59.714282	66.451009
1399.922259	50.192845	66.456014
1399.064478	64.916949	66.461018
1398.648605	58.426357	66.466023
1398.213168	57.407515	66.471028
1397.037920	57.304169	66.476033
1396.361575	56.853453	66.481038
1395.679889	65.740324	66.486042
1395.484530	57.371304	66.491047
1394.966082	64.997527	66.496052
1393.533238	59.179496	66.501057
1392.876578	56.201058	66.506062
1392.317123	56.556474	66.511066
1392.427731	46.976661	66.516071
1391.567750	62.623591	66.521076
1390.776782	58.006042	66.526081
1390.404172	54.801113	66.531086
1389.330940	60.750986	66.536090
1388.205489	60.305429	66.541095
1387.846391	49.652304	66.546100
1387.434277	61.069800	66.551105
1387.178599	49.285378	66.556110
1386.100996	62.518000	66.561114
1385.587106	63.290356	66.566119
1384.915095	53.879094	66.571124
1383.795037	63.909506	66.576129
1383.186206	59.805456	66.581134
1382.261914	68.861777	66.586138
1382.004378	60.527870	66.591143
1381.694813	69.670972	66.596148
1380.794280	67.533936	66.601153
1380.306829	61.743824	66.606158
1379.635882	58.196828	66.611162
1379.061111	63.249069	66.616167
1377.930959	65.713617	66.621172
1376.869886	52.768904	66.626177
1376.693626	52.066820	66.631182
1376.284425	64.078341	66.636186
1376.073633	63.641932	66.641191
1374.660748	68.161954	66.646196
1373.897242	61.124256	66.651201
1373.666338	58.940702	66.656206
1372.808802	64.862602	66.661210
1371.548215	63.009876	66.666215
1371.073997	57.050515	66.671220
1370.663875	59.946212	66.676225
1370.241801	62.362859	66.681230
1370.081125	68.426290	66.686234
1369.180532	65.256408	66.691239
1368.249249	66.456224	66.696244
1367.809651	65.070634	66.701249
1367.016800	61.033686	66.706254
1365.864694	65.307262	66.711258
1365.317031	55.398443	66.716263
1365.112568	60.890115	66.721268
1364.447488	66.537008	66.726273
1363.921869	64.133809	66.731278
1362.914131	58.535215	66.736282
1362.432499	55.798610	66.741287
1361.366190	60.883260	66.746292
1360.214252	69.931621	66.751297
1360.117060	56.661810	66.756302
1359.405693	61.216972	66.761306
1359.585647	58.684269	66.766311
1358.494629	57.246122	66.771316
1358.019301	61.092009	66.776321
1357.497632	55.220617	66.781326
1356.059025	63.682216	66.786330
1355.276585	63.182147	66.791335
1354.914363	63.591369	66.796340
1353.909357	60.767661	66.801345
1353.902641	58.510625	66.806350
1352.864344	58.429682	66.811354
1352.246433	63.332673	66.816359
1351.616999	54.718865	66.821364
1351.078091	65.708686	66.826369
1350.542087	53.095239	66.831374
1349.399752	70.035960	66.836378
1348.893611	66.710344	66.841383
1348.649005	56.849542	66.846388
1348.270442	59.738648	66.851393
1347.265738	44.140563	66.856398
1346.387991	61.723581	66.861402
1345.878350	50.086769	66.866407
1344.534120	55.761206	66.871412
1343.822864	55.932615	66.876417
1343.511882	48.763074	66.881422
1343.091266	57.769290	66.886426
1342.623717	48.049588	66.891431
1342.009314	56.999880	66.896436
1341.072819	53.364231	66.901441
1340.669107	63.410082	66.906446
1340.168723	59.465416	66.911450
1339.289904	55.197729	66.916455
1338.517977	59.358840	66.921460
1337.763303	58.449103	66.926465
1337.439286	53.084012	66.931470
1336.265643	57.528172	66.936474
1335.800412	58.581372	66.941479
1335.523971	54.243155	66.946484
1334.569178	57.953965	66.951489
1333.714324	57.079078	66.956494
1332.501213	59.418067	66.961498
1332.291697	54.052120	66.966503
1332.008683	57.206723	66.971508
1331.421369	56.779715	66.976513
1330.577648	57.033685	66.981518
1329.844291	56.107947	66.986522
1329.495303	55.151064	66.991527
1329.120664	49.076542	66.996532
1327.705780	49.918033	67.001537
1327.559332	51.844608	67.006542
1326.351222	54.741021	67.011546
1325.173952	48.097119	67.016551
1324.814368	44.628371	67.021556
1324.057444	58.393471	67.026561
1324.024455	38.332877	67.031566
1323.533554	54.802610	67.036570
1323.265888	44.641150	67.041575
1322.156503	44.830129	67.046580
1321.318781	59.000720	67.051585
1321.088581	39.778842	67.056590
1319.778112	41.743822	67.061594
1319.039725	51.623686	67.066599
1318.584963	47.433666	67.071604
1318.074034	53.393509	67.076609
1317.681736	40.050794	67.081614
1316.576417	50.872048	67.086618
1316.055324	48.083384	67.091623
1315.742664	53.464528	67.096628
1314.850851	49.917976	67.101633
1314.095955	40.869993	67.106638
1313.249792	49.320991	67.111642
1312.831512	41.917795	67.116647
1311.868537	38.439328	67.121652
1310.966347	48.796222	67.126657
1310.663633	48.415432	67.131662
1310.347715	45.122663	67.136666
1309.707165	40.635769	67.141671
1308.729291	41.802013	67.146676
1307.919852	56.602013	67.151681
1307.481676	50.256911	67.156686
1306.852742	49.869642	67.161690
1306.055393	42.649709	67.166695
1305.481570	51.681858	67.171700
1304.958369	49.054373	67.176705
1304.333513	46.222288	67.181710
1303.079597	55.032996	67.186714
1302.496528	52.077577	67.191719
1302.264947	58.535459	67.196724
1301.717655	62.077419	67.201729
1300.710887	56.937572	67.206734
1299.870868	50.629554	67.211738
1299.416572	52.023205	67.216743
1298.887071	47.827725	67.221748
1298.420843	51.202261	67.226753
1297.612775	56.583327	67.231758
1296.878772	59.997285	67.236762
1296.327865	46.752324	67.241767
1295.212658	55.470022	67.246772
1294.355213	52.080432	67.251777
1294.081215	45.406472	67.256782
1293.548734	47.615187	67.261786
1293.278187	50.580160	67.266791
1292.865129	50.841362	67.271796
1291.836293	58.179750	67.276801
1291.753598	49.037512	67.281806
1290.015577	51.404784	67.286810
1289.593015	48.119511	67.291815
1289.229021	46.520076	67.296820
1288.501135	52.501802	67.301825
1287.751695	52.128966	67.306830
1286.666463	50.836582	67.311834
1286.650141	43.941890	67.316839
1285.326646	44.462958	67.321844
1284.281564	43.678256	67.326849
1284.507463	45.083605	67.331854
1283.698424	54.536338	67.336858
1283.336443	53.625680	67.341863
1282.356990	47.559026	67.346868
1281.613590	52.948736	67.351873
1281.435603	43.902074	67.356878
1279.968335	49.920938	67.361882
1279.438148	51.213123	67.366887
1278.815962	49.465515	67.371892
1278.448638	53.574924	67.376897
1278.372524	49.335747	67.381902
1277.063560	51.494466	67.386906
1276.229355	52.078086	67.391911
1275.896543	46.635564	67.396916
1274.734480	54.761503	67.401921
1274.304594	42.829778	67.406926
1273.591018	52.637901	67.411930
1273.240401	46.316733	67.416935
1272.950600	45.692632	67.421940
1271.750750	57.235377	67.426945
1271.338529	37.129444	67.431950
1270.562167	51.061631	67.436954
1269.674786	56.726539	67.441959
1268.974039	48.991387	67.446964
1267.836807	45.591104	67.451969
1267.601789	44.958293	67.456974
1267.293543	50.007592	67.461978
1266.962899	48.745040	67.466983
1265.986215	44.852474	67.471988
1264.825136	54.711254	67.476993
1264.881638	43.367639	67.481998
1263.790441	53.863405	67.487002
1262.762502	50.262827	67.492007
1262.328471	40.952544	67.497012
1261.469088	44.525208	67.502017
1261.265945	44.530697	67.507022
1260.834206	49.093453	67.512026
1260.026224	50.961221	67.517031
1259.408760	53.337990	67.522036
1258.724090	44.852845	67.527041
1257.800483	52.888837	67.532046
1256.696356	49.623637	67.537050
1256.489090	49.696011	67.542055
1256.654330	38.297266	67.547060
1255.026116	55.143372	67.552065
1254.820172	42.069074	67.557070
1254.166288	43.937570	67.562074
1253.486695	41.421695	67.567079
1252.452657	36.653627	67.572084
1251.648044	52.685984	67.577089
1251.247689	50.606657	67.582094
1250.561829	48.938563	67.587098
1250.002316	50.257493	67.592103
1249.390634	47.036992	67.597108
1248.702221	44.298603	67.602113
1248.566541	46.753301	67.607118
1247.285459	49.197747	67.612122
1246.592716	40.653971	67.617127
1246.028766	40.669526	67.622132
1245.468187	50.442286	67.627137
1244.574691	43.947263	67.632142
1243.612930	57.309725	67.637146
1243.262122	46.440865	67.642151
1242.979458	53.674811	67.647156
1242.122659	55.372159	67.652161
1241.599218	42.949141	67.657166
1240.538605	56.294207	67.662170
1239.956787	49.989308	67.667175
1240.111767	52.869277	67.672180
1238.247699	55.281856	67.677185
1238.214766	48.183236	67.682190
1237.455746	57.169155	67.687194
1236.658831	56.095862	67.692199
1235.976139	55.311899	67.697204
1235.231198	47.937009	67.702209
1235.005599	43.023048	67.707214
1234.426933	62.313594	67.712218
1233.599789	60.638009	67.717223
1232.910632	48.622946	67.722228
1232.126286	56.405001	67.727233
1231.444281	49.042179	67.732238
1230.399032	43.559998	67.737242
1230.141622	50.950768	67.742247
1229.619864	54.619560	67.747252
1229.021276	47.793807	67.752257
1228.300992	42.118033	67.757262
1227.306268	50.501216	67.762266
1226.730609	37.425798	67.767271
1226.668215	46.493316	67.772276
1225.166991	44.797199	67.777281
1224.899006	43.463192	67.782286
1223.980493	54.029277	67.787290
1223.511316	39.968720	67.792295
1223.063123	34.355334	67.797300
1221.709672	53.337008	67.802305
1221.503756	52.060937	67.807310
1220.866246	40.502852	67.812314
1220.780449	51.605116	67.817319
1219.789126	50.583244	67.822324
1218.603176	47.953942	67.827329
1218.406388	47.712430	67.832334
1217.680886	51.265395	67.837338
1216.603995	51.173299	67.842343
1216.089813	49.630873	67.847348
1215.651912	48.268696	67.852353
1215.405135	47.637760	67.857358
1214.364643	48.750921	67.862362
1213.776214	50.774591	67.867367
1213.148272	56.343068	67.872372
1212.314498	63.049673	67.877377
1211.726355	46.084493	67.882382
1210.716150	63.248647	67.887386
1210.431855	44.579423	67.892391
1210.101367	54.429135	67.897396
1208.770815	52.524544	67.902401
1208.376597	56.811695	67.907406
1207.648678	46.157349	67.912410
1207.249541	47.997962	67.917415
1206.402350	54.044408	67.922420
1205.911602	55.429679	67.927425
1205.835328	42.831489	67.932430
1204.610620	56.401346	67.937434
1203.701684	55.755868	67.942439
1203.271474	58.892890	67.947444
1201.984532	59.714103	67.952449
1201.464540	50.348118	67.957454
1201.066453	49.388024	67.962458
1200.518702	48.043319	67.967463
1200.264371	49.614911	67.972468
1199.151054	47.360404	67.977473
1198.460014	52.699231	67.982478
1197.820692	45.288637	67.987482
1197.324628	56.631180	67.992487
1196.271939	50.439021	67.997492
1195.532589	55.345582	68.002497
1194.787796	54.890036	68.007502
1194.568354	45.700177	68.012506
1193.968936	50.267531	68.017511
1193.088446	53.047249	68.022516
1192.383519	47.290199	68.027521
1192.353980	46.206845	68.032526
1190.958223	45.574138	68.037530
1190.371647	51.131308	68.042535
1190.014357	48.438044	68.047540
1189.126581	51.154269	68.052545
1188.877276	41.428293	68.057550
1187.593514	47.539440	68.062554
1187.309403	44.139135	68.067559
1186.936281	46.879165	68.072564
1185.749011	53.489032	68.077569
1185.263056	44.010415	68.082574
1184.436142	44.911434	68.087578
1184.197174	41.198037	68.092583
1183.401386	49.407676	68.097588
1181.918584	57.647734	68.102593
1182.069051	46.224530	68.107598
1181.414519	55.168611	68.112602
1180.766182	49.161302	68.117607
1179.921227	33.500072	68.122612
1179.225667	43.977090	68.127617
1179.099696	46.674661	68.132622
1177.949725	40.190495	68.137626
1176.760451	46.860603	68.142631
1176.559734	42.761095	68.147636
1175.688734	52.370353	68.152641
1175.787742	44.645236	68.157646
1174.561571	54.028718	68.162650
1173.818053	47.483064	68.167655
1173.489813	39.825898	68.172660
1172.978641	47.581862	68.177665
1172.564613	53.573620	68.182670
1171.387705	53.953168	68.187674
1170.660595	55.368151	68.192679
1170.126406	39.230162	68.197684
1168.825226	49.719928	68.202689
1168.473978	49.096150	68.207694
1167.784263	50.804794	68.212698
1167.837237	41.041787	68.217703
1167.149017	40.488947	68.222708
1166.235695	48.102299	68.227713
1165.723532	41.313284	68.232718
1164.893701	46.812955	68.237722
1163.914905	49.081638	68.242727
1163.350350	45.579288	68.247732
1162.726328	46.175246	68.252737
1162.499140	46.944623	68.257742
1161.363829	52.492881	68.262746
1160.730027	52.451758	68.267751
1160.388261	47.392287	68.272756
1159.504085	60.412864	68.277761
1158.710742	37.909230	68.282766
1157.863588	60.438809	68.287770
1157.308759	52.756178	68.292775
1157.040527	53.237207	68.297780
1156.363923	53.727994	68.302785
1155.574733	41.665802	68.307790
1154.615488	55.248646	68.312794
1154.659199	35.382469	68.317799
1153.722639	44.920157	68.322804
1152.299035	49.952899	68.327809
1152.350006	45.073807	68.332814
1151.592073	45.702103	68.337818
1150.875527	49.214238	68.342823
1149.756738	50.290994	68.347828
1149.122408	49.893584	68.352833
1149.210337	41.604131	68.357838
1148.791019	49.531562	68.362842
1147.688253	46.773953	68.367847
1147.135899	37.879896	68.372852
1146.235831	47.268287	68.377857
1145.907798	37.542229	68.382862
1144.808550	44.338372	68.387866
1144.241699	45.672682	68.392871
1143.562179	43.254594	68.397876
1143.090185	40.693118	68.402881
1142.353894	35.212302	68.407886
1141.410559	50.811018	68.412890
1140.885723	47.898417	68.417895
1140.951318	37.559423	68.422900
1139.425914	47.321652	68.427905
1138.944295	48.848979	68.432910
1138.278313	45.755411	68.437914
1137.939850	46.293341	68.442919
1137.074424	41.640426	68.447924
1136.167078	51.018941	68.452929
1135.936669	45.601158	68.457934
1135.141579	43.277144	68.462938
1134.280933	46.873700	68.467943
1133.525115	48.162378	68.472948
1132.731278	47.672076	68.477953
1132.790825	45.872842	68.482958
1131.545329	42.433078	68.487962
1130.847114	47.402492	68.492967
1130.612050	45.339472	68.497972
1129.785000	53.133071	68.502977
1129.467770	42.566395	68.507982
1128.152778	62.812958	68.512986
1127.727484	44.013231	68.517991
1127.476321	46.555682	68.522996
1126.524429	47.435599	68.528001
1125.711282	39.768842	68.533006
1124.958523	55.051839	68.538010
1124.682975	46.298251	68.543015
1124.029919	45.995284	68.548020
1122.940835	41.366910	68.553025
1122.643163	31.501998	68.558030
1122.035522	48.384513	68.563034
1121.505240	42.084071	68.568039
1120.777136	36.128896	68.573044
1119.904369	54.515355	68.578049
1119.047341	41.640837	68.583054
1118.139953	59.924005	68.588058
1117.858956	41.509745	68.593063
1117.564126	41.581866	68.598068
1116.667716	48.194378	68.603073
1115.532512	41.163872	68.608078
1114.758080	52.873955	68.613082
1114.239063	48.724162	68.618087
1114.103200	49.799123	68.623092
1113.441139	48.370123	68.628097
1112.715976	44.208968	68.633102
1112.009180	41.915071	68.638106
1111.266551	47.528612	68.643111
1110.982847	49.320916	68.648116
1109.887059	48.205323	68.653121
1109.613749	46.623029	68.658126
1108.822814	45.659210	68.663130
1107.513977	58.115015	68.668135
1107.142180	43.094453	68.673140
1106.507332	42.544179	68.678145
1106.594848	47.212007	68.683150
1105.496245	44.229839	68.688154
1104.668855	42.253156	68.693159
1104.064366	45.820013	68.698164
1103.195608	50.871752	68.703169
1102.297547	36.005869	68.708174
1101.474392	55.472486	68.713178
1101.122310	45.242503	68.718183
1100.955504	48.071145	68.723188
1100.523552	53.097558	68.728193
1100.023231	37.400468	68.733198
1098.911846	47.680305	68.738202
1098.446175	46.287876	68.743207
1097.229022	39.961089	68.748212
1096.593419	41.243270	68.753217
1096.017875	46.775046	68.758222
1095.546500	54.658727	68.763226
1094.525411	49.398257	68.768231
1093.874296	45.135448	68.773236
1093.188120	48.852490	68.778241
1093.240272	30.402605	68.783246
1092.214437	50.294097	68.788250
1091.185098	41.491698	68.793255
1090.975793	41.939707	68.798260
1090.060548	43.957044	68.803265
1089.484028	42.970162	68.808270
1088.426541	52.728948	68.813274
1087.702461	54.550307	68.818279
1087.695523	37.811265	68.823284
1086.978422	51.327219	68.828289
1086.445730	47.029804	68.833294
1085.399445	47.891637	68.838298
1084.724697	43.635744	68.843303
1084.567551	41.752715	68.848308
1083.653246	46.739167	68.853313
1082.970977	34.101790	68.858318
1082.372898	40.469742	68.863322
1081.568174	36.519942	68.868327
1080.847776	40.237698	68.873332
1079.903830	43.793907	68.878337
1079.562242	39.393561	68.883342
1079.134565	38.043976	68.888346
1078.280162	43.227470	68.893351
1077.564285	40.121359	68.898356
1076.894974	36.342399	68.903361
1076.861762	41.481991	68.908366
1075.471030	41.204924	68.913370
1074.931629	44.051839	68.918375
1074.596586	38.409450	68.923380
1073.176570	37.397487	68.928385
1072.798953	29.486441	68.933390
1072.166795	38.087941	68.938394
1071.776955	49.318977	68.943399
1071.301863	38.225523	68.948404
1070.199718	32.385059	68.953409
1069.663091	33.531658	68.958414
1068.948279	35.064553	68.963418
1068.485782	46.950512	68.968423
1067.512883	31.434268	68.973428
1066.771030	43.657962	68.978433
1066.485396	35.528864	68.983438
1065.947356	46.258373	68.988442
1065.028567	49.572478	68.993447
1064.445843	33.410720	68.998452
1063.828887	43.151464	69.003457
1063.162782	42.038498	69.008462
1062.012856	41.915510	69.013466
1061.258386	33.110403	69.018471
1060.890370	36.671187	69.023476
1060.819166	41.878320	69.028481
1060.442967	36.816465	69.033486
1059.090330	44.613266	69.038490
1058.394440	46.001236	69.043495
1058.026893	30.932721	69.048500
1056.868984	47.918545	69.053505
1056.297696	25.613041	69.058510
1055.875272	42.384090	69.063514
1055.719338	33.149471	69.068519
1054.676930	40.860652	69.073524
1053.769337	46.490988	69.078529
1053.308976	36.669315	69.083534
1051.544574	44.015986	69.088538
1051.399715	41.504985	69.093543
1051.152749	31.099038	69.098548
1050.376717	50.108746	69.103553
1050.476139	30.498650	69.108558
1049.579841	41.933248	69.113562
1048.717572	40.148205	69.118567
1048.282323	28.780357	69.123572
1046.689463	51.428563	69.128577
1046.184185	46.639542	69.133582
1045.554756	41.400365	69.138586
1045.274469	45.021309	69.143591
1044.865505	42.684781	69.148596
1043.630430	40.129611	69.153601
1043.171071	30.695697	69.158606
1042.797149	41.424326	69.163610
1042.265404	35.956733	69.168615
1041.445939	40.481852	69.173620
1040.120111	48.744308	69.178625
1040.026888	40.344917	69.183630
1039.602796	44.261538	69.188634
1038.968729	51.042061	69.193639
1038.198836	35.507725	69.198644
1037.347419	50.155173	69.203649
1036.557485	39.654264	69.208654
1035.801255	49.803508	69.213658
1035.370664	41.331639	69.218663
1035.253110	39.511698	69.223668
1033.764124	49.039539	69.228673
1033.115905	36.503992	69.233678
1032.549643	50.010146	69.238682
1031.990423	52.850761	69.243687
1031.918755	41.473949	69.248692
1030.341837	43.345851	69.253697
1030.096727	43.786945	69.258702
1029.427497	42.712330	69.263706
1028.731130	33.926376	69.268711
1027.812035	33.755642	69.273716
1027.116900	52.785600	69.278721
1026.641525	33.706900	69.283726
1026.402127	48.993382	69.288730
1025.702842	49.596616	69.293735
1024.827042	40.109112	69.298740
1023.779637	49.565128	69.303745
1023.564002	40.598616	69.308750
1022.337386	47.771442	69.313754
1021.827530	44.493805	69.318759
1021.954132	37.450250	69.323764
1021.089446	43.302416	69.328769
1020.133466	47.792494	69.333774
1019.766867	44.427414	69.338778
1019.022909	37.978080	69.343783
1018.034112	45.854203	69.348788
1016.973351	47.811142	69.353793
1016.693030	39.829433	69.358798
1016.383637	44.990887	69.363802
1016.039099	36.648831	69.368807
1014.711503	36.839546	69.373812
1013.681213	49.531746	69.378817
1013.540543	34.553295	69.383822
1013.182765	44.429422	69.388826
1011.885639	38.050754	69.393831
1011.287257	29.895739	69.398836
1010.786895	53.089199	69.403841
1010.426508	39.115481	69.408846
1009.768894	51.491360	69.413850
1008.739675	51.491110	69.418855
1008.493302	42.162078	69.423860
1007.987090	42.712522	69.428865
1006.964586	41.829731	69.433870
1006.376853	44.148209	69.438874
1005.655284	42.206761	69.443879
1004.710052	41.083030	69.448884
1003.446020	38.455222	69.453889
1003.244152	34.018469	69.458894
1002.460019	42.224713	69.463898
1002.326354	43.226792	69.468903
1002.604417	45.234064	69.473908
1001.324198	41.203834	69.478913
1000.731199	46.594907	69.483918
999.805805	46.983400	69.488922
998.350544	43.080365	69.493927
997.851881	52.026480	69.498932
997.483447	50.298493	69.503937
997.373529	46.846848	69.508942
996.819982	40.073927	69.513946
995.805726	38.563809	69.518951
995.371355	34.159319	69.523956
994.324336	53.261036	69.528961
993.756106	38.473610	69.533966
992.794957	47.994754	69.538970
992.143590	36.820568	69.543975
992.007713	44.896866	69.548980
991.362007	38.127573	69.553985
990.590401	39.817752	69.558990
989.722761	38.085622	69.563994
988.995181	47.858173	69.568999
987.908267	34.783771	69.574004
987.169565	45.972548	69.579009
987.117877	39.584957	69.584014
986.695498	52.896345	69.589018
986.415152	41.339864	69.594023
985.683795	46.973717	69.599028
984.560200	35.138271	69.604033
983.565500	43.685514	69.609038
982.759224	43.591458	69.614042
981.980739	56.394987	69.619047
982.079962	43.817793	69.624052
981.189120	47.043903	69.629057
981.061646	39.933547	69.634062
979.895109	33.898380	69.639066
979.218431	45.720654	69.644071
978.342282	34.746236	69.649076
977.597871	39.215277	69.654081
977.364871	38.134342	69.659086
976.210352	51.013468	69.664090
976.154122	35.449183	69.669095
975.816116	46.410210	69.674100
974.584302	41.717890	69.679105
974.371867	44.708330	69.684110
973.043509	34.928603	69.689114
971.946561	41.577791	69.694119
971.544685	36.870106	69.699124
971.059138	38.448546	69.704129
970.928899	39.867953	69.709134
970.357373	44.435639	69.714138
969.168816	52.748822	69.719143
968.648313	42.425831	69.724148
968.237447	46.411317	69.729153
967.237052	34.726580	69.734158
966.727798	38.883830	69.739162
965.968121	42.481715	69.744167
965.268983	34.065214	69.749172
964.251045	35.401955	69.754177
963.880987	39.362023	69.759182
963.514628	38.955135	69.764186
962.797231	46.483753	69.769191
962.034008	37.569695	69.774196
961.138748	42.128972	69.779201
960.763101	40.977701	69.784206
960.385097	35.367401	69.789210
959.611902	40.965339	69.794215
958.700966	37.172826	69.799220
958.241599	46.109535	69.804225
957.030532	34.937696	69.809230
956.389677	41.462279	69.814234
955.644125	37.337537	69.819239
955.400970	35.020373	69.824244
955.080395	36.946283	69.829249
954.437059	40.445238	69.834254
953.557805	45.541263	69.839258
952.920313	40.197747	69.844263
952.320769	35.436369	69.849268
951.013061	52.152765	69.854273
950.698209	44.804158	69.859278
950.625871	45.634063	69.864282
949.617121	44.335965	69.869287
948.876699	44.234595	69.874292
948.411564	55.781958	69.879297
947.429228	41.670692	69.884302
946.494626	50.383420	69.889306
945.527313	54.304499	69.894311
945.368865	47.225880	69.899316
944.952404	50.527896	69.904321
944.699179	35.078538	69.909326
943.426479	53.227476	69.914330
942.843862	56.242135	69.919335
942.628588	37.661366	69.924340
941.065286	52.595570	69.929345
940.958713	47.235377	69.934350
939.905308	42.046353	69.939354
939.398105	46.955452	69.944359
939.461592	45.855724	69.949364
938.279290	51.895646	69.954369
937.813440	43.577638	69.959374
937.245180	44.642570	69.964378
935.814864	48.438642	69.969383
935.550325	37.805287	69.974388
934.683243	44.410027	69.979393
934.532986	37.295420	69.984398
933.400745	49.089277	69.989402
932.741038	50.369025	69.994407
932.245547	42.516185	69.999412
931.694239	45.111143	70.004417
931.368360	36.007660	70.009422
930.239847	45.899212	70.014426
929.812916	44.133240	70.019431
929.308006	50.566816	70.024436
928.220050	44.743083	70.029441
927.575312	44.383653	70.034446
926.775433	48.073099	70.039450
926.375220	40.432169	70.044455
925.735685	53.202555	70.049460
924.685403	39.754943	70.054465
924.328481	40.652212	70.059470
923.913117	36.213175	70.064474
923.069655	47.909043	70.069479
922.491645	50.251223	70.074484
921.802157	47.322301	70.079489
921.388973	48.237985	70.084494
920.050486	50.272274	70.089498
919.311585	55.521011	70.094503
919.008238	60.501751	70.099508
918.422610	53.413846	70.104513
918.064927	50.547234	70.109518
917.092685	58.537448	70.114522
916.063277	48.153537	70.119527
915.911385	46.017385	70.124532
915.301871	62.788267	70.129537
914.669305	52.724382	70.134542
913.913389	47.976857	70.139546
913.256947	51.865821	70.144551
912.357341	51.143274	70.149556
911.186458	50.120140	70.154561
910.651761	40.028075	70.159566
910.483044	42.396580	70.164570
910.225954	48.964175	70.169575
909.416087	55.589782	70.174580
908.449246	55.489765	70.179585
908.149676	49.843335	70.184590
907.325582	55.810496	70.189594
906.312474	51.722039	70.194599
905.911711	47.477789	70.199604
905.188570	59.843616	70.204609
904.897024	50.698398	70.209614
903.801297	53.241238	70.214618
903.002748	42.776446	70.219623
902.623041	52.343850	70.224628
902.128874	57.474800	70.229633
901.355465	42.283264	70.234638
900.704467	55.307779	70.239642
899.753365	49.981071	70.244647
899.648407	42.225353	70.249652
898.409410	48.231736	70.254657
898.000059	49.624607	70.259662
897.708522	57.779295	70.264666
896.329997	51.665943	70.269671
895.435392	48.476374	70.274676
895.019620	67.021951	70.279681
894.714731	52.189486	70.284686
894.233960	55.593202	70.289690
893.058140	53.642082	70.294695
892.926013	47.536945	70.299700
892.174955	60.314051	70.304705
891.696226	56.932146	70.309710
890.428514	55.919701	70.314714
889.874460	49.347151	70.319719
889.733603	50.298343	70.324724
888.623946	50.667318	70.329729
888.125554	44.986308	70.334734
887.460352	51.221483	70.339738
886.720867	50.214855	70.344743
885.844168	43.457127	70.349748
884.638189	45.322118	70.354753
884.345672	45.125830	70.359758
883.969568	51.781751	70.364762
883.628306	41.464953	70.369767
883.154961	48.495876	70.374772
881.945422	43.442109	70.379777
881.784959	43.237419	70.384782
881.019762	40.481401	70.389786
879.955626	38.674933	70.394791
879.397513	49.432887	70.399796
878.443795	49.532633	70.404801
878.703197	30.646122	70.409806
877.446290	44.320545	70.414810
876.660302	48.405165	70.419815
876.841871	44.943407	70.424820
875.418067	43.541096	70.429825
874.278829	49.391270	70.434830
873.801672	46.195193	70.439834
873.458206	45.429878	70.444839
873.344561	48.398293	70.449844
871.948359	41.042043	70.454849
871.086066	38.536437	70.459854
871.136857	54.155176	70.464858
870.478151	46.968539	70.469863
869.407818	41.094726	70.474868
868.555392	54.532905	70.479873
868.045657	47.630050	70.484878
867.961415	46.804556	70.489882
867.183502	58.493165	70.494887
866.680978	48.080613	70.499892
865.932087	46.679693	70.504897
865.124432	50.353048	70.509902
863.974376	44.324776	70.514906
863.738975	41.623207	70.519911
863.320885	46.537057	70.524916
862.083743	44.061153	70.529921
861.404476	43.399746	70.534926
860.913203	49.312368	70.539930
860.318247	45.627289	70.544935
859.132429	39.516408	70.549940
858.525926	53.339627	70.554945
857.973030	43.975835	70.559950
857.465835	48.101239	70.564954
857.220738	55.169953	70.569959
857.013687	50.278323	70.574964
855.419885	53.644742	70.579969
855.329555	52.178429	70.584974
854.896426	47.814768	70.589978
853.380257	48.421916	70.594983
852.606605	48.843077	70.599988
852.391774	55.749287	70.604993
851.875608	50.039576	70.609998
850.678340	51.512132	70.615002
849.761970	45.954426	70.620007
849.797787	43.501412	70.625012
849.147401	54.734507	70.630017
848.671165	49.042094	70.635022
847.935790	52.006971	70.640026
846.939453	47.878027	70.645031
846.895125	52.032258	70.650036
846.058122	57.132633	70.655041
845.002165	47.055745	70.660046
844.531592	45.151663	70.665050
843.818703	47.415983	70.670055
842.927979	46.282062	70.675060
841.972205	42.479385	70.680065
841.912747	53.512773	70.685070
841.364918	53.861726	70.690074
840.514714	56.791270	70.695079
839.926253	40.933269	70.700084
839.376849	47.384975	70.705089
838.802447	44.800442	70.710094
837.490527	47.324106	70.715098
836.753059	47.379986	70.720103
836.857078	40.351067	70.725108
836.164582	45.111487	70.730113
834.971619	48.913985	70.735118
834.555497	44.806230	70.740122
833.765108	48.527305	70.745127
833.753522	48.757791	70.750132
832.572013	52.522200	70.755137
832.165420	50.037107	70.760142
831.377327	44.127848	70.765146
829.980713	61.511272	70.770151
829.787759	43.966136	70.775156
829.030172	47.410769	70.780161
829.026559	46.671786	70.785166
828.015750	49.866580	70.790170
826.988226	45.069285	70.795175
827.137240	45.159096	70.800180
825.981440	47.090241	70.805185
825.042420	45.243382	70.810190
824.271188	49.650504	70.815194
824.037322	43.493765	70.820199
823.855485	47.387622	70.825204
822.758787	51.160611	70.830209
822.159571	43.076742	70.835214
821.569578	53.117571	70.840218
820.372589	45.933058	70.845223
819.654593	43.784528	70.850228
819.116632	55.240993	70.855233
818.896046	49.962034	70.860238
818.205304	53.437030	70.865242
816.803546	49.194445	70.870247
816.598864	44.512169	70.875252
816.022660	42.337917	70.880257
815.664267	47.131889	70.885262
814.774809	45.595673	70.890266
813.702734	41.798907	70.895271
813.653535	43.475065	70.900276
812.784484	45.600256	70.905281
812.368064	43.283881	70.910286
811.592059	55.032115	70.915290
810.578681	48.740851	70.920295
810.251277	34.992170	70.925300
808.989224	52.485051	70.930305
808.645552	44.877723	70.935310
808.450389	44.304842	70.940314
807.691540	53.544693	70.945319
806.562570	37.294956	70.950324
805.663565	58.954498	70.955329
805.260538	40.081971	70.960334
804.996808	44.665342	70.965338
804.443349	46.366580	70.970343
803.458057	49.440633	70.975348
802.573437	41.930455	70.980353
802.279223	43.339703	70.985358
801.731379	47.657657	70.990362
800.709316	44.764368	70.995367
800.459008	47.538507	71.000372
799.682443	54.067381	71.005377
798.970311	51.839079	71.010382
797.910883	48.817704	71.015386
797.442299	42.915941	71.020391
797.517303	35.374431	71.025396
796.482273	50.942083	71.030401
795.689171	43.067274	71.035406
795.138313	44.586759	71.040410
794.111213	46.932647	71.045415
793.405825	39.468057	71.050420
792.458188	46.085659	71.055425
792.112754	52.318834	71.060430
792.082358	41.561508	71.065434
790.617130	49.977145	71.070439
789.961527	34.986102	71.075444
789.628609	54.354211	71.080449
789.601165	35.421907	71.085454
788.573848	41.862969	71.090458
787.572982	41.560267	71.095463
787.268904	40.686198	71.100468
785.566012	52.624561	71.105473
784.873640	50.189701	71.110478
784.656429	43.585639	71.115482
784.022652	51.102560	71.120487
784.076029	44.233083	71.125492
783.516796	53.578350	71.130497
782.944724	45.357715	71.135502
782.181950	37.312514	71.140506
781.210182	47.291123	71.145511
780.330317	36.501883	71.150516
779.588552	52.178965	71.155521
779.308334	48.500571	71.160526
778.644684	45.786765	71.165530
777.563119	53.103751	71.170535
777.323247	46.299880	71.175540
776.004069	47.151667	71.180545
775.312689	40.820201	71.185550
774.541184	52.239733	71.190554
773.985862	50.782797	71.195559
774.133088	46.087080	71.200564
773.558377	56.734157	71.205569
772.725145	51.871263	71.210574
772.260920	48.135435	71.215578
771.086278	58.351344	71.220583
770.270490	51.760574	71.225588
769.418856	53.832547	71.230593
768.948453	47.136335	71.235598
768.699526	46.672937	71.240602
768.060938	46.785632	71.245607
767.109646	49.338648	71.250612
766.009514	51.609446	71.255617
766.115369	40.486675	71.260622
765.564871	37.942509	71.265626
764.201677	40.263070	71.270631
763.955819	45.034400	71.275636
763.106971	54.050479	71.280641
762.767688	43.675051	71.285646
761.721351	43.460019	71.290650
761.119820	56.572865	71.295655
761.001644	39.402184	71.300660
759.838410	54.689076	71.305665
759.214439	46.292216	71.310670
758.811689	59.296152	71.315674
758.319769	56.878270	71.320679
757.380531	35.102957	71.325684
756.138946	50.705079	71.330689
755.879608	41.375008	71.335694
755.449009	36.132652	71.340698
754.173943	46.968489	71.345703
753.889666	47.053164	71.350708
753.205914	46.610109	71.355713
752.825413	40.735334	71.360718
752.317013	47.283022	71.365722
751.288054	44.302547	71.370727
750.863884	49.081767	71.375732
749.934238	54.800859	71.380737
749.057563	43.191146	71.385742
748.527283	32.327346	71.390746
748.036296	49.528760	71.395751
748.124861	42.374578	71.400756
746.657670	54.485162	71.405761
745.837347	41.420488	71.410766
745.638089	53.360748	71.415770
744.745299	44.003800	71.420775
743.706497	41.220429	71.425780
743.281270	42.702577	71.430785
742.998639	46.497372	71.435790
742.528172	44.973320	71.440794
741.371657	45.386088	71.445799
741.167622	42.367320	71.450804
740.164572	40.972213	71.455809
739.251124	44.466913	71.460814
738.768361	43.088316	71.465818
737.820571	45.582439	71.470823
737.318900	45.720650	71.475828
736.142220	53.314554	71.480833
735.713202	42.071948	71.485838
735.249548	37.665870	71.490842
734.733010	44.307890	71.495847
734.733472	48.500715	71.500852
733.515028	52.792991	71.505857
732.960310	48.210607	71.510862
732.286338	46.681113	71.515866
731.675320	52.158678	71.520871
730.991302	44.889392	71.525876
729.979814	42.823885	71.530881
729.656799	46.169394	71.535886
728.979736	50.582047	71.540890
727.505067	48.434175	71.545895
727.010466	41.618833	71.550900
726.503003	48.125376	71.555905
726.350801	40.618465	71.560910
726.364008	44.005055	71.565914
725.229862	52.677079	71.570919
724.442996	45.862540	71.575924
723.428003	40.547661	71.580929
722.710837	37.925969	71.585934
722.219092	42.846829	71.590938
721.218873	49.710934	71.595943
721.408467	39.945138	71.600948
720.418113	50.374556	71.605953
719.811558	38.070606	71.610958
719.257416	40.103112	71.615962
718.384935	47.114027	71.620967
717.687522	38.039786	71.625972
716.908379	45.494709	71.630977
716.471457	48.788974	71.635982
715.395892	41.600958	71.640986
714.526737	49.778230	71.645991
714.262575	36.781135	71.650996
713.743674	48.355988	71.656001
713.242867	41.153728	71.661006
712.410217	45.845033	71.666010
711.794260	54.010378	71.671015
711.503313	37.201517	71.676020
709.921542	55.779765	71.681025
709.478347	48.878973	71.686030
708.999136	48.447516	71.691034
708.193848	53.656412	71.696039
708.066461	40.651730	71.701044
707.051253	50.653047	71.706049
706.314252	51.082609	71.711054
706.011565	45.914507	71.716058
704.858478	50.242118	71.721063
704.116716	39.404115	71.726068
703.481771	41.862631	71.731073
702.957494	46.845442	71.736078
702.897484	41.528321	71.741082
701.863091	38.723768	71.746087
701.411737	56.559090	71.751092
700.541314	44.593607	71.756097
700.109644	47.412399	71.761102
699.069242	50.044279	71.766106
698.285069	60.347846	71.771111
698.057325	37.853759	71.776116
696.969384	50.875330	71.781121
696.224778	37.013345	71.786126
695.839575	43.443656	71.791130
694.991970	45.057717	71.796135
695.033289	37.909485	71.801140
693.524413	43.758663	71.806145
693.178854	38.229981	71.811150
692.832638	38.630438	71.816154
691.415478	49.842145	71.821159
691.218605	29.921344	71.826164
690.189780	44.713783	71.831169
689.789077	41.357349	71.836174
689.509557	36.907771	71.841178
688.620440	48.453270	71.846183
688.036678	32.663975	71.851188
687.419479	46.578787	71.856193
686.855828	49.655126	71.861198
685.905881	41.173011	71.866202
685.316302	51.481858	71.871207
684.839234	43.001713	71.876212
683.765502	39.588451	71.881217
682.980272	41.763411	71.886222
682.493940	32.535735	71.891226
681.953858	33.227246	71.896231
681.535155	42.382993	71.901236
680.589566	37.221079	71.906241
679.967723	34.793946	71.911246
679.898152	34.114350	71.916250
678.784868	40.130767	71.921255
678.216887	42.424092	71.926260
677.389608	38.072774	71.931265
676.475049	36.496456	71.936270
675.530471	36.022419	71.941274
674.780389	38.038828	71.946279
674.958069	32.663365	71.951284
674.221864	38.320133	71.956289
673.397876	45.048963	71.961294
672.330243	33.766153	71.966298
671.849862	42.707807	71.971303
671.627937	31.197298	71.976308
670.843632	43.177092	71.981313
670.251510	35.241951	71.986318
669.287097	38.993933	71.991322
668.967240	42.706354	71.996327
668.462683	34.042949	72.001332
667.251810	45.037321	72.006337
666.492413	43.974011	72.011342
666.283955	28.102892	72.016346
665.241941	44.671415	72.021351
664.450259	39.524422	72.026356
663.730843	37.090754	72.031361
663.782408	37.831552	72.036366
663.402011	42.051905	72.041370
661.955558	41.399184	72.046375
661.400052	39.693160	72.051380
660.905724	36.536135	72.056385
660.494551	41.778470	72.061390
659.526558	38.731562	72.066394
658.798265	34.993661	72.071399
658.687009	24.749110	72.076404
657.516122	36.935532	72.081409
656.944922	30.679586	72.086414
656.428812	38.357548	72.091418
655.437666	33.448893	72.096423
654.705967	36.138857	72.101428
653.743839	31.665529	72.106433
653.593268	30.446929	72.111438
653.482317	34.540800	72.116442
652.215516	47.874699	72.121447
651.430866	32.191522	72.126452
651.184661	34.097738	72.131457
649.999747	41.746594	72.136462
649.481111	28.635513	72.141466
648.740674	43.380460	72.146471
648.226520	29.650531	72.151476
647.619161	41.256816	72.156481
647.027431	39.050388	72.161486
646.509987	38.943560	72.166490
645.659090	47.251975	72.171495
645.237164	33.106832	72.176500
644.189943	50.412594	72.181505
643.525399	41.438796	72.186510
643.126366	48.092077	72.191514
642.197628	41.233936	72.196519
641.586890	35.810569	72.201524
640.607117	37.259624	72.206529
640.350946	41.969526	72.211534
640.102710	38.353868	72.216538
639.227578	29.202314	72.221543
638.214351	35.753137	72.226548
637.859675	33.162051	72.231553
637.331950	41.291274	72.236558
636.324622	33.994670	72.241562
635.469501	38.938718	72.246567
635.562441	31.213022	72.251572
634.375714	40.584114	72.256577
633.480716	38.167378	72.261582
633.543745	31.383107	72.266586
632.064991	41.945512	72.271591
631.228048	34.180253	72.276596
630.560789	34.348008	72.281601
630.220394	39.733607	72.286606
629.979626	43.323056	72.291610
629.382583	39.423921	72.296615
628.938064	27.540464	72.301620
628.145899	37.011138	72.306625
627.168876	36.908121	72.311630
626.220756	28.767931	72.316634
625.226530	33.797208	72.321639
625.085943	34.756253	72.326644
624.486333	36.012314	72.331649
624.228748	45.374207	72.336654
623.368517	35.990060	72.341658
622.406209	40.760381	72.346663
622.281475	33.728482	72.351668
621.157119	37.523298	72.356673
620.407996	33.615272	72.361678
620.147920	31.974167	72.366682
619.341418	39.827684	72.371687
618.396807	36.316625	72.376692
617.392703	31.747501	72.381697
616.954681	28.570483	72.386702
616.801813	38.290989	72.391706
616.323805	46.399685	72.396711
615.809945	41.042892	72.401716
614.955833	38.493503	72.406721
613.797653	34.467708	72.411726
613.103812	30.673877	72.416730
612.202539	40.445770	72.421735
611.978518	33.499067	72.426740
611.330268	41.986515	72.431745
610.934976	40.650781	72.436750
610.183139	38.477746	72.441754
609.259166	38.304789	72.446759
608.497081	39.348623	72.451764
607.559946	41.882094	72.456769
606.938966	43.590971	72.461774
606.817149	42.022460	72.466778
606.032487	37.856760	72.471783
605.785154	32.971586	72.476788
604.662878	44.915337	72.481793
604.299528	42.044954	72.486798
603.719604	32.100539	72.491802
602.431234	49.246030	72.496807
602.215874	32.899806	72.501812
601.542852	48.181202	72.506817
600.286740	42.362338	72.511822
599.854004	36.190005	72.516826
599.128503	43.503954	72.521831
599.138442	43.193301	72.526836
598.350003	38.657641	72.531841
597.416057	37.697842	72.536846
596.934192	38.198760	72.541850
596.064322	33.829028	72.546855
595.561867	38.422045	72.551860
594.211565	39.844980	72.556865
594.046354	38.728058	72.561870
593.949159	36.840253	72.566874
592.775866	46.131957	72.571879
591.813753	38.616870	72.576884
591.040009	46.384760	72.581889
590.889068	43.370168	72.586894
590.539701	41.552486	72.591898
589.273082	46.882192	72.596903
589.343381	30.283909	72.601908
588.455038	40.422735	72.606913
587.733564	42.961286	72.611918
586.643272	43.639530	72.616922
585.915658	44.405082	72.621927
585.768916	42.430556	72.626932
584.562963	47.096201	72.631937
584.094621	43.197079	72.636942
583.553548	44.759201	72.641946
583.066803	40.407296	72.646951
582.201878	41.003917	72.651956
581.352514	52.533651	72.656961
580.942169	29.780133	72.661966
580.483926	34.011314	72.666970
579.719978	33.197902	72.671975
579.215247	35.172106	72.676980
578.086216	41.668861	72.681985
577.418738	35.177549	72.686990
576.590418	27.188605	72.691994
575.801250	46.138948	72.696999
575.863952	37.347374	72.702004
575.414841	37.625471	72.707009
574.935734	34.067094	72.712014
573.907923	42.504622	72.717018
573.070349	52.267964	72.722023
572.044377	44.386182	72.727028
571.369469	45.502870	72.732033
570.928963	43.854240	72.737038
570.878553	40.104587	72.742042
569.585448	36.562326	72.747047
568.754842	43.200777	72.752052
568.031380	41.518373	72.757057
567.792275	42.756449	72.762062
567.432094	42.630897	72.767066
566.002498	46.346628	72.772071
565.812655	28.394257	72.777076
564.838347	44.579879	72.782081
564.598383	40.967644	72.787086
563.661504	41.113710	72.792090
562.967857	46.044677	72.797095
562.976714	38.745513	72.802100
562.087390	48.170186	72.807105
561.053404	43.935409	72.812110
560.366038	38.139516	72.817114
559.750833	52.375708	72.822119
559.309466	45.930380	72.827124
558.221698	46.832149	72.832129
557.509037	51.047095	72.837134
557.470852	49.727026	72.842138
556.140673	40.955471	72.847143
555.659354	30.998522	72.852148
554.696579	47.070354	72.857153
554.379215	36.328812	72.862158
554.555843	38.470445	72.867162
553.382521	44.632084	72.872167
552.521020	37.867349	72.877172
551.782023	47.537724	72.882177
550.947933	48.534700	72.887182
550.293054	44.103932	72.892186
549.758578	46.965927	72.897191
549.609193	47.823881	72.902196
548.529279	41.874486	72.907201
547.730098	36.821766	72.912206
547.261635	44.389659	72.917210
546.585880	38.356967	72.922215
546.005068	44.924099	72.927220
544.815795	44.569509	72.932225
544.534060	31.620989	72.937230
544.440953	34.682323	72.942234
543.529148	46.326079	72.947239
542.594921	42.679362	72.952244
541.955803	43.995350	72.957249
541.367159	39.054168	72.962254
540.618642	32.446476	72.967258
539.355386	45.713620	72.972263
539.346315	39.708770	72.977268
538.638591	43.987583	72.982273
538.053077	42.948653	72.987278
537.287130	34.446765	72.992282
536.386392	41.714527	72.997287
536.398721	41.471298	73.002292
535.187027	45.655357	73.007297
534.444697	37.115016	73.012302
533.928408	43.310768	73.017306
533.137663	47.782571	73.022311
532.854871	42.631831	73.027316
532.008254	43.080482	73.032321
531.454759	44.075344	73.037326
531.248271	36.640185	73.042330
530.356931	38.352723	73.047335
529.516636	36.636905	73.052340
528.811406	42.142126	73.057345
528.099012	49.886067	73.062350
527.104916	44.735099	73.067354
526.169395	44.455208	73.072359
526.498398	41.070874	73.077364
525.868212	47.445612	73.082369
524.753976	45.754509	73.087374
524.288205	37.048699	73.092378
523.440096	43.535417	73.097383
522.255158	48.003788	73.102388
521.489607	42.734419	73.107393
521.127454	40.858864	73.112398
521.102737	27.770069	73.117402
520.370720	48.064268	73.122407
519.878871	39.480877	73.127412
518.973164	53.224061	73.132417
518.347264	39.609736	73.137422
517.363976	39.132465	73.142426
516.252582	43.095562	73.147431
515.825182	37.877981	73.152436
515.219400	45.532403	73.157441
515.221208	47.679806	73.162446
514.931267	37.408542	73.167450
513.769658	39.897383	73.172455
513.326823	30.982933	73.177460
512.063757	39.426417	73.182465
511.219177	41.915217	73.187470
510.798361	39.060312	73.192474
509.993728	43.844976	73.197479
509.717601	36.061388	73.202484
508.335374	41.605077	73.207489
507.763957	31.725569	73.212494
507.817027	46.102871	73.217498
507.128654	48.409103	73.222503
506.905346	40.654944	73.227508
505.961852	47.743458	73.232513
505.010384	43.525523	73.237518
504.551037	52.285661	73.242522
503.015582	47.468510	73.247527
503.259947	34.310040	73.252532
502.525268	41.543474	73.257537
501.524825	52.457083	73.262542
501.162558	37.290130	73.267546
500.222380	56.657191	73.272551
499.755974	39.193559	73.277556
498.664391	47.843112	73.282561
497.999006	44.945173	73.287566
497.648634	38.862239	73.292570
496.736680	46.287911	73.297575
496.919760	39.768354	73.302580
495.648580	36.112261	73.307585
495.021460	41.756426	73.312590
494.686789	40.218677	73.317594
493.786347	40.084590	73.322599
493.006406	28.544753	73.327604
492.272393	43.474768	73.332609
491.918247	38.207678	73.337614
491.282554	44.553339	73.342618
490.459071	39.903459	73.347623
489.846504	38.310640	73.352628
489.241204	44.181553	73.357633
488.133459	42.971955	73.362638
487.811587	39.306551	73.367642
486.969068	45.062300	73.372647
486.663758	37.240790	73.377652
485.633091	39.950044	73.382657
484.964124	35.188824	73.387662
484.481316	41.428132	73.392666
483.894295	41.803905	73.397671
483.592241	33.985032	73.402676
482.571519	43.824872	73.407681
481.693437	49.337144	73.412686
480.984010	40.652816	73.417690
480.068136	48.033388	73.422695
479.761273	40.126975	73.427700
479.267745	41.705196	73.432705
478.625788	42.857657	73.437710
478.327772	33.864953	73.442714
476.828397	49.946602	73.447719
476.505919	46.011651	73.452724
476.032952	36.154311	73.457729
474.993207	36.736245	73.462734
474.617482	30.993231	73.467738
473.744295	41.479736	73.472743
473.539972	37.059211	73.477748
472.629946	45.506392	73.482753
471.759295	47.245616	73.487758
471.423646	39.892540	73.492762
470.619327	47.023543	73.497767
469.915900	34.262065	73.502772
468.994311	41.798081	73.507777
468.281465	45.784431	73.512782
468.328315	41.241892	73.517786
467.282902	46.809210	73.522791
466.779198	40.484220	73.527796
465.862010	41.385659	73.532801
465.522138	39.222727	73.537806
464.493555	37.789229	73.542810
463.448925	45.909369	73.547815
463.235051	44.904284	73.552820
462.935010	52.574659	73.557825
462.290634	41.506787	73.562830
461.731694	32.724383	73.567834
460.514320	44.079390	73.572839
460.564764	46.398806	73.577844
459.323545	56.967612	73.582849
458.366089	37.707335	73.587854
458.168894	43.451736	73.592858
457.175816	42.476182	73.597863
456.501805	38.190412	73.602868
456.050946	44.188104	73.607873
455.328817	51.265020	73.612878
455.424449	39.279781	73.617882
454.115254	50.739307	73.622887
453.532255	34.144206	73.627892
453.012122	45.405477	73.632897
452.157557	38.969244	73.637902
451.211603	39.291830	73.642906
450.415992	44.492942	73.647911
450.290881	40.747313	73.652916
449.714172	44.191611	73.657921
448.970699	41.805996	73.662926
448.437254	38.795593	73.667930
447.739258	36.450039	73.672935
446.679480	35.715340	73.677940
445.827331	47.838444	73.682945
445.761977	45.880922	73.687950
445.080167	36.265012	73.692954
443.871783	47.769975	73.697959
443.356749	40.283069	73.702964
442.877609	42.423523	73.707969
442.341094	44.101635	73.712974
441.480988	43.704111	73.717978
440.695668	38.322812	73.722983
440.173301	41.965023	73.727988
439.850838	55.375615	73.732993
438.604323	42.255995	73.737998
437.976345	44.681923	73.743002
437.391542	55.548253	73.748007
437.444482	46.685703	73.753012
436.513637	51.354887	73.758017
435.528198	46.435957	73.763022
435.316859	40.427073	73.768026
434.159784	54.330168	73.773031
433.387640	41.360463	73.778036
432.747313	48.995174	73.783041
432.310319	48.877149	73.788046
431.772441	39.145274	73.793050
430.569841	54.377038	73.798055
430.134481	43.178108	73.803060
429.683767	42.936121	73.808065
429.401005	40.540181	73.813070
428.314818	44.347918	73.818074
427.299492	52.805585	73.823079
427.391592	43.682923	73.828084
426.680825	47.317311	73.833089
425.188170	45.479979	73.838094
425.112261	34.914453	73.843098
424.174262	44.398950	73.848103
424.005429	34.322867	73.853108
422.772465	39.052805	73.858113
421.974865	45.061597	73.863118
421.887201	36.309762	73.868122
421.109447	44.256514	73.873127
420.645384	32.289504	73.878132
419.639448	35.223488	73.883137
419.054549	38.971853	73.888142
418.879186	42.490972	73.893146
417.553763	43.389669	73.898151
416.864053	32.428388	73.903156
416.260837	39.334980	73.908161
416.112384	39.008566	73.913166
415.291709	36.966405	73.918170
414.215847	42.533861	73.923175
413.858643	29.912775	73.928180
413.197921	40.285019	73.933185
412.293470	40.908496	73.938190
411.809758	36.608187	73.943194
411.346696	45.324768	73.948199
411.048158	38.587079	73.953204
409.977873	30.833866	73.958209
409.375529	47.540542	73.963214
408.424097	30.783409	73.968218
407.355764	43.486559	73.973223
407.161414	42.571403	73.978228
406.518639	47.951591	73.983233
406.147861	53.468203	73.988238
405.244040	42.134204	73.993242
404.167011	44.671114	73.998247
403.835364	38.900590	74.003252
403.458007	43.320749	74.008257
402.480550	42.678601	74.013262
401.719570	37.687655	74.018266
401.007890	35.530366	74.023271
401.160224	32.330283	74.028276
399.643697	44.950321	74.033281
398.829704	37.861130	74.038286
398.522797	31.541073	74.043290
398.236778	46.486445	74.048295
397.702608	37.501426	74.053300
396.502768	36.710224	74.058305
396.067303	44.299680	74.063310
395.558261	42.785001	74.068314
394.330025	43.210934	74.073319
393.755727	40.910337	74.078324
392.875695	36.728375	74.083329
392.484906	39.398776	74.088334
392.547576	25.613297	74.093338
391.281537	40.293803	74.098343
390.523011	41.526358	74.103348
390.056589	44.371230	74.108353
389.393749	49.518089	74.113358
388.460570	36.085242	74.118362
387.751978	40.430457	74.123367
387.611984	39.639098	74.128372
387.377090	39.906746	74.133377
386.435098	50.923030	74.138382
385.454767	38.831724	74.143386
384.507686	37.891447	74.148391
383.793924	34.107171	74.153396
382.984783	38.271301	74.158401
382.372286	44.706320	74.163406
381.941025	37.384270	74.168410
381.459827	45.438307	74.173415
381.368674	33.404002	74.178420
380.426283	43.857405	74.183425
379.698593	47.675841	74.188430
378.875946	41.583038	74.193434
377.618595	45.757097	74.198439
377.294669	37.000342	74.203444
376.765374	37.983495	74.208449
376.321049	38.180445	74.213454
375.448708	37.285028	74.218458
374.655091	59.834525	74.223463
374.514246	43.129567	74.228468
373.711415	45.200195	74.233473
372.516584	50.682555	74.238478
371.843543	43.121505	74.243482
371.620831	39.736770	74.248487
371.460106	33.475419	74.253492
370.301844	43.863883	74.258497
369.351853	40.115678	74.263502
369.205029	39.859966	74.268506
368.007593	44.429735	74.273511
367.513136	48.045436	74.278516
366.712417	50.670788	74.283521
366.193194	43.837392	74.288526
365.974326	42.025757	74.293530
365.149587	52.764757	74.298535
364.572278	40.454703	74.303540
363.784108	43.776606	74.308545
362.403975	49.673254	74.313550
362.341373	36.227835	74.318554
361.582313	49.591308	74.323559
361.145896	32.961851	74.328564
360.266406	35.669137	74.333569
359.612553	43.416394	74.338574
359.299507	45.306479	74.343578
358.122560	54.643009	74.348583
357.894235	37.657128	74.353588
357.034844	45.618481	74.358593
356.511709	52.151225	74.363598
355.715746	42.750645	74.368602
354.465919	48.158202	74.373607
354.156768	35.556278	74.378612
353.685621	32.222176	74.383617
353.242585	42.884574	74.388622
352.376968	44.332892	74.393626
351.358310	31.654817	74.398631
351.059706	30.144458	74.403636
350.577669	48.247989	74.408641
349.598116	41.533688	74.413646
349.076033	39.138054	74.418650
348.405601	43.795725	74.423655
347.949454	43.597193	74.428660
346.878696	31.187607	74.433665
346.158498	39.924670	74.438670
346.221186	39.613494	74.443674
344.930336	39.663098	74.448679
344.443705	38.930138	74.453684
343.756740	36.693239	74.458689
343.323150	42.932605	74.463694
342.509714	35.527977	74.468698
341.462197	35.940904	74.473703
340.904989	41.302735	74.478708
340.616851	42.420918	74.483713
339.967503	44.717818	74.488718
338.919252	46.274090	74.493722
338.271895	45.566746	74.498727
338.337790	35.472191	74.503732
337.386895	39.592697	74.508737
336.318133	46.428428	74.513742
335.891576	39.588160	74.518746
334.939615	36.742251	74.523751
334.644895	40.472771	74.528756
334.010607	40.903418	74.533761
333.165458	43.509052	74.538766
332.788055	42.153171	74.543770
331.906323	55.922536	74.548775
331.165400	40.836479	74.553780
330.534860	45.454682	74.558785
329.920118	44.587609	74.563790
329.293312	36.177164	74.568794
328.108315	50.734407	74.573799
327.942973	36.791309	74.578804
327.254096	43.730493	74.583809
327.151799	46.183048	74.588814
326.192586	39.661049	74.593818
325.185965	41.029352	74.598823
324.897559	43.834825	74.603828
323.769231	51.296610	74.608833
323.082591	51.190008	74.613838
322.955445	39.645541	74.618842
322.035539	54.781826	74.623847
321.299641	32.168603	74.628852
320.742375	47.584533	74.633857
320.073931	42.069540	74.638862
319.510446	39.861851	74.643866
318.268498	44.916526	74.648871
318.013513	46.297496	74.653876
317.490905	43.657538	74.658881
316.900317	40.719350	74.663886
316.058532	40.851930	74.668890
314.827483	55.268296	74.673895
314.803694	44.541516	74.678900
314.622948	42.895689	74.683905
313.532937	37.935140	74.688910
313.039908	40.923028	74.693914
311.787967	42.765649	74.698919
310.604233	43.346947	74.703924
310.332219	45.959009	74.708929
309.851243	50.376771	74.713934
309.592098	42.100109	74.718938
308.965765	39.268540	74.723943
308.742503	43.030249	74.728948
307.773220	42.131385	74.733953
306.769722	46.358052	74.738958
306.144523	44.287928	74.743962
304.744261	39.785238	74.748967
304.299351	41.234324	74.753972
304.171484	45.565846	74.758977
304.009002	40.862723	74.763982
302.939012	40.129714	74.768986
301.903264	50.238497	74.773991
301.584239	36.802421	74.778996
301.293961	41.293861	74.784001
300.135620	49.039542	74.789006
299.489526	43.017974	74.794010
298.912415	39.456358	74.799015
298.444367	39.105201	74.804020
297.213115	40.550316	74.809025
296.728239	39.883314	74.814030
296.337556	25.608741	74.819034
295.563385	42.762250	74.824039
295.403691	38.769850	74.829044
294.616479	32.657246	74.834049
293.451367	43.373239	74.839054
292.580713	39.522540	74.844058
291.645148	40.586234	74.849063
291.258626	38.471765	74.854068
291.101973	44.633883	74.859073
290.777829	46.372788	74.864078
289.793138	44.429349	74.869082
288.596372	45.384875	74.874087
288.282723	39.836996	74.879092
287.596584	35.562675	74.884097
286.927042	41.801810	74.889102
286.309255	36.021728	74.894106
285.520099	41.543534	74.899111
285.274494	42.331686	74.904116
284.664201	51.027598	74.909121
283.343326	38.467107	74.914126
283.272367	34.060043	74.919130
282.401912	34.927292	74.924135
281.679801	37.254725	74.929140
281.282589	48.923750	74.934145
280.487991	41.836246	74.939150
280.064073	36.190835	74.944154
278.740335	47.709514	74.949159
278.099540	28.901904	74.954164
277.541847	44.007258	74.959169
277.479615	36.218007	74.964174
276.407280	43.052751	74.969178
275.244850	45.029348	74.974183
275.391659	45.067441	74.979188
274.923240	30.652305	74.984193
273.701903	32.160502	74.989198
273.119343	43.173131	74.994202
272.438219	41.255425	74.999207
271.780006	42.738516	75.004212
270.664639	43.542311	75.009217
270.275576	44.143610	75.014222
270.067368	43.632775	75.019226
269.299548	48.935157	75.024231
268.464030	32.657915	75.029236
267.911974	52.805187	75.034241
267.450022	38.467859	75.039246
266.789966	40.323384	75.044250
265.526599	40.474298	75.049255
265.445595	41.468014	75.054260
264.439543	41.445457	75.059265
263.391501	38.676390	75.064270
262.913116	30.822599	75.069274
262.376283	32.857167	75.074279
262.146087	37.408413	75.079284
261.478788	41.672964	75.084289
260.627515	35.821304	75.089294
260.430542	37.978308	75.094298
259.078713	41.957759	75.099303
258.134499	45.422830	75.104308
257.690026	37.844312	75.109313
257.311341	38.757753	75.114318
257.180620	26.584710	75.119322
256.008535	32.385167	75.124327
255.328412	37.690915	75.129332
254.621782	31.537098	75.134337
253.626386	38.848410	75.139342
253.102493	28.709118	75.144346
252.485802	37.489620	75.149351
252.056640	33.781440	75.154356
251.665676	28.742608	75.159361
250.895760	37.381964	75.164366
250.375068	34.700720	75.169370
249.326434	40.374278	75.174375
248.581715	34.210765	75.179380
247.857529	46.108519	75.184385
246.768307	44.478211	75.189390
246.666809	28.605920	75.194394
246.342653	44.047765	75.199399
245.572632	30.770329	75.204404
244.588614	30.778959	75.209409
244.074570	45.103119	75.214414
243.858275	42.158899	75.219418
242.335886	40.570837	75.224423
241.859139	36.498105	75.229428
241.420789	32.015576	75.234433
240.924642	30.301770	75.239438
240.377013	30.393792	75.244442
239.586075	47.633560	75.249447
238.866454	41.628464	75.254452
238.093143	32.173871	75.259457
237.139785	37.431720	75.264462
236.894215	34.616742	75.269466
236.264136	39.214389	75.274471
234.850743	29.926486	75.279476
234.385490	31.829808	75.284481
233.878762	35.127380	75.289486
233.709255	27.684803	75.294490
233.147762	36.538504	75.299495
232.404835	32.714776	75.304500
231.457436	35.150671	75.309505
231.098327	34.785315	75.314510
230.173917	40.500573	75.319514
229.035588	48.362933	75.324519
228.817400	36.036684	75.329524
228.073215	36.614179	75.334529
227.732135	45.812774	75.339534
227.065026	37.765159	75.344538
226.062362	47.800885	75.349543
225.720198	38.987150	75.354548
224.827403	38.640643	75.359553
224.040929	41.883471	75.364558
223.593976	30.864648	75.369562
222.938233	40.036135	75.374567
222.575347	35.596769	75.379572
221.550892	36.919073	75.384577
221.017264	36.810184	75.389582
220.729388	34.240058	75.394586
219.330710	39.775474	75.399591
218.747154	28.081458	75.404596
218.324823	39.997319	75.409601
217.818745	31.343754	75.414606
217.049237	34.749449	75.419610
215.918655	42.104403	75.424615
215.710990	40.901244	75.429620
215.219443	32.366782	75.434625
214.184902	39.227058	75.439630
213.779445	35.428379	75.444634
212.974845	53.947594	75.449639
212.638286	39.150349	75.454644
211.387900	44.996425	75.459649
210.653206	48.547954	75.464654
210.323985	33.702239	75.469658
209.783847	36.153636	75.474663
209.403596	37.190329	75.479668
208.616674	40.023249	75.484673
207.639214	36.657940	75.489678
207.304933	29.490780	75.494682
205.845178	56.515962	75.499687
205.577289	40.916184	75.504692
205.123008	38.639078	75.509697
204.465950	40.110963	75.514702
203.935292	30.693390	75.519706
203.206197	43.025568	75.524711
202.294349	37.375966	75.529716
202.145549	33.023893	75.534721
200.879244	36.109848	75.539726
200.535133	29.119288	75.544730
199.746799	41.542907	75.549735
199.417057	38.586819	75.554740
198.765071	42.246581	75.559745
198.126388	41.727116	75.564750
197.715024	34.666855	75.569754
196.154430	42.631235	75.574759
195.720708	37.512502	75.579764
195.135131	31.497093	75.584769
194.294218	46.232893	75.589774
193.314591	40.169923	75.594778
192.414866	46.970873	75.599783
192.371933	35.807223	75.604788
192.077940	43.829856	75.609793
191.831390	46.314873	75.614798
191.086886	35.408145	75.619802
190.142995	42.807457	75.624807
189.473922	44.169305	75.629812
188.335494	31.827364	75.634817
187.571040	45.035611	75.639822
187.399672	36.819094	75.644826
186.599867	40.942371	75.649831
185.631966	44.226750	75.654836
184.895374	39.813857	75.659841
184.355737	50.264603	75.664846
184.280349	25.623965	75.669850
183.006161	33.544263	75.674855
182.320632	42.695277	75.679860
181.882692	41.579294	75.684865
181.353270	53.769271	75.689870
181.446941	34.652224	75.694874
180.645334	50.160734	75.699879
179.590232	35.760319	75.704884
178.426804	33.173683	75.709889
177.442866	47.336236	75.714894
177.359990	38.963694	75.719898
176.695815	45.285571	75.724903
176.265599	43.553381	75.729908
175.416013	42.126160	75.734913
174.503975	35.830088	75.739918
174.273592	38.437098	75.744922
173.139379	53.077754	75.749927
172.524111	38.154657	75.754932
171.784463	45.854130	75.759937
171.331697	41.459064	75.764942
171.419841	38.078407	75.769946
169.849315	45.591827	75.774951
169.340136	39.468054	75.779956
168.999587	40.719184	75.784961
168.128533	43.638065	75.789966
167.424281	32.139917	75.794970
166.534322	42.837314	75.799975
166.207794	38.824222	75.804980
165.896717	42.109535	75.809985
164.697054	45.476604	75.814990
164.118880	38.282106	75.819994
163.528050	41.670366	75.824999
162.986791	38.741701	75.830004
162.070712	44.840409	75.835009
161.371357	43.168479	75.840014
160.845116	44.520176	75.845018
159.720199	47.708182	75.850023
158.894444	47.185440	75.855028
158.667643	44.406899	75.860033
158.090385	56.746424	75.865038
157.948797	40.317591	75.870042
157.442575	45.750168	75.875047
156.290277	41.337338	75.880052
155.962106	42.308968	75.885057
154.623637	49.779091	75.890062
154.087264	45.643349	75.895066
153.249845	43.195543	75.900071
153.054397	45.741796	75.905076
152.592128	37.420288	75.910081
151.346433	56.675279	75.915086
151.046593	51.585664	75.920090
150.474728	49.663187	75.925095
149.337030	55.155456	75.930100
148.639265	41.350901	75.935105
147.953099	40.682910	75.940110
148.005484	32.506415	75.945114
147.094107	52.518602	75.950119
146.083814	43.100249	75.955124
145.597750	41.394316	75.960129
145.115943	41.838543	75.965134
144.562133	42.076645	75.970138
143.249765	55.616685	75.975143
143.030773	49.643753	75.980148
142.573896	43.032280	75.985153
141.601488	41.356589	75.990158
141.057899	42.096080	75.995162
140.676595	41.346368	76.000167
140.243840	44.867115	76.005172
138.727277	37.500571	76.010177
137.913860	49.187082	76.015182
137.883016	36.931900	76.020186
137.333681	42.715109	76.025191
136.347715	38.307305	76.030196
135.578246	43.603674	76.035201
134.995723	35.828018	76.040206
134.831286	31.953082	76.045210
133.594296	39.500064	76.050215
132.901737	41.269347	76.055220
132.514183	36.516983	76.060225
131.845300	56.455821	76.065230
131.027843	48.537858	76.070234
130.182483	49.749645	76.075239
129.822515	31.457110	76.080244
129.326020	43.190849	76.085249
128.094548	42.455283	76.090254
127.742364	36.937233	76.095258
126.928001	45.247837	76.100263
126.820890	34.349882	76.105268
125.961571	35.877691	76.110273
124.800104	34.725711	76.115278
124.477156	31.587215	76.120282
123.939763	41.465204	76.125287
123.248816	37.185395	76.130292
122.587207	35.121129	76.135297
121.774976	46.389584	76.140302
121.610479	35.264251	76.145306
120.141445	38.483491	76.150311
119.568986	45.033591	76.155316
119.285501	36.150606	76.160321
118.774953	43.450880	76.165326
118.033114	30.369271	76.170330
117.075346	33.801859	76.175335
116.679541	42.849919	76.180340
116.408279	37.558651	76.185345
114.987564	45.010368	76.190350
114.770652	38.415830	76.195354
114.326391	39.853806	76.200359
113.462683	43.243015	76.205364
112.462169	46.417511	76.210369
111.857278	41.993103	76.215374
111.448921	30.793127	76.220378
110.201781	45.456532	76.225383
109.552345	36.098925	76.230388
109.547264	36.389873	76.235393
108.810295	38.109477	76.240398
108.176381	33.484709	76.245402
107.280124	50.646680	76.250407
106.780573	49.950520	76.255412
106.443676	43.457111	76.260417
105.323512	48.744761	76.265422
104.537837	39.580756	76.270426
103.906771	41.721842	76.275431
103.144379	41.493348	76.280436
102.565981	33.827427	76.285441
101.665087	43.339209	76.290446
101.319407	34.213849	76.295450
100.865551	37.982378	76.300455
100.040472	34.542358	76.305460
98.795566	43.528715	76.310465
98.434028	42.482562	76.315470
98.343085	32.908174	76.320474
97.736078	42.839843	76.325479
96.831237	44.876363	76.330484
96.218152	34.562118	76.335489
95.788199	35.288228	76.340494
94.805041	39.377694	76.345498
94.011709	34.546553	76.350503
93.698003	38.390499	76.355508
93.169026	27.113579	76.360513
91.782308	44.818932	76.365518
91.449868	36.542966	76.370522
90.520436	37.848593	76.375527
90.425364	29.629390	76.380532
89.566222	31.250217	76.385537
88.463518	36.080950	76.390542
88.491541	26.727279	76.395546
87.542752	43.889739	76.400551
86.790969	32.642040	76.405556
86.235491	34.551891	76.410561
85.626903	40.825498	76.415566
85.065859	41.356485	76.420570
83.864284	43.828238	76.425575
83.392976	43.439798	76.430580
82.984207	28.091180	76.435585
82.099309	44.257915	76.440590
81.512211	32.730081	76.445594
80.490255	39.299831	76.450599
80.223982	42.522817	76.455604
79.956848	40.912864	76.460609
79.070710	46.715104	76.465614
78.320010	31.446243	76.470618
77.637284	34.718296	76.475623
77.167940	39.981008	76.480628
76.418772	42.047899	76.485633
75.669777	35.265426	76.490638
75.110636	31.749891	76.495642
73.928793	35.152001	76.500647
73.362227	30.622154	76.505652
72.922198	43.045441	76.510657
72.470979	39.284049	76.515662
72.151183	36.476198	76.520666
70.770860	42.373019	76.525671
70.259536	37.630946	76.530676
69.985310	28.386975	76.535681
68.977938	48.591086	76.540686
68.091396	35.478958	76.545690
67.668992	34.726352	76.550695
67.167959	37.731326	76.555700
66.276650	34.316072	76.560705
65.529008	37.847625	76.565710
65.068194	30.251269	76.570714
64.320002	32.171359	76.575719
64.024785	32.656802	76.580724
63.258488	36.243367	76.585729
62.358881	39.304022	76.590734
62.107870	34.186143	76.595738
60.563985	41.364233	76.600743
60.058755	37.269280	76.605748
59.566406	35.753592	76.610753
59.067181	47.112482	76.615758
59.094163	24.600088	76.620762
57.709121	36.628490	76.625767
57.040714	40.459627	76.630772
56.680785	31.013296	76.635777
55.823501	38.747321	76.640782
55.036327	23.717671	76.645786
54.347508	42.541681	76.650791
54.130727	33.449389	76.655796
53.449729	33.066014	76.660801
52.101005	45.383505	76.665806
52.353371	33.609842	76.670810
50.982298	38.081293	76.675815
49.951517	39.973921	76.680820
49.597812	33.401212	76.685825
48.999568	41.439259	76.690830
48.981749	31.578844	76.695834
48.299591	45.267545	76.700839
47.332612	37.655729	76.705844
46.761933	32.170968	76.710849
45.969049	45.513075	76.715854
45.525231	23.317033	76.720858
44.369651	46.236479	76.725863
43.823992	39.678615	76.730868
43.040588	32.546850	76.735873
41.829896	37.147258	76.740878
41.531170	38.117360	76.745882
40.937925	31.273794	76.750887
40.752753	34.455463	76.755892
40.700795	39.508116	76.760897
39.751341	38.563623	76.765902
38.827388	32.124442	76.770906
38.028447	41.217881	76.775911
37.233329	43.298419	76.780916
36.334257	37.228984	76.785921
35.840766	36.352111	76.790926
35.649805	33.589947	76.795930
34.589809	44.344458	76.800935
33.954174	36.739722	76.805940
33.178635	31.281332	76.810945
32.788835	35.291951	76.815950
32.231900	34.849373	76.820954
31.340856	32.621466	76.825959
30.899166	35.500293	76.830964
30.544033	34.852075	76.835969
28.958590	42.981350	76.840974
28.650439	34.961707	76.845978
27.992715	42.463651	76.850983
27.430125	37.122675	76.855988
26.544545	30.346239	76.860993
25.790376	39.203894	76.865998
25.910959	46.651085	76.871002
24.958465	40.659556	76.876007
23.955845	49.276163	76.881012
23.340346	30.874621	76.886017
22.851895	33.478650	76.891022
22.674655	33.268809	76.896026
21.385516	35.540103	76.901031
20.589402	44.191576	76.906036
20.368285	34.395126	76.911041
19.253402	40.156599	76.916046
18.499726	39.740673	76.921050
17.820393	35.889530	76.926055
17.745481	41.379481	76.931060
17.332834	37.132585	76.936065
16.048817	36.632525	76.941070
15.400220	32.855324	76.946074
14.860721	45.368593	76.951079
14.008056	24.431457	76.956084
13.459677	32.004261	76.961089
12.303616	42.581724	76.966094
12.153830	38.832188	76.971098
11.580095	36.985736	76.976103
11.275086	38.991262	76.981108
10.527747	41.313332	76.986113
9.480706	37.654874	76.991118
8.881235	29.426254	76.996122
7.542849	37.817312	77.001127
7.591516	38.877078	77.006132
7.114949	34.605690	77.011137
6.311509	37.312000	77.016142
6.095942	33.864677	77.021147
4.993383	32.181420	77.026151
4.615943	38.446555	77.031156
3.749736	25.864204	77.036161