Mon Mar 08 19:01:15 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.381347	102.241253	0.000000
0.097996	87.260480	0.005005
-1.006879	63.238153	0.010010
-2.084334	8.726111	0.015014
-6.116544	-13.380030	0.020019
-11.458538	-18.385974	0.025024
-16.473686	-16.586308	0.030029
-21.157594	-8.565170	0.035034
-25.016805	-13.463852	0.040038
-28.823214	-2.521998	0.045043
-32.247250	-9.035404	0.050048
-35.777099	-12.075462	0.055053
-39.879536	-4.680019	0.060058
-43.552659	-13.525259	0.065062
-47.720789	-11.688769	0.070067
-51.239001	-15.780843	0.075072
-54.777255	-6.529542	0.080077
-58.497908	-11.390353	0.085082
-62.115326	-0.838122	0.090086
-66.097849	-7.112582	0.095091
-70.152818	-12.560243	0.100096
-73.389984	-7.519840	0.105101
-77.512641	-6.923652	0.110106
-81.034343	-20.443122	0.115110
-84.909848	-16.346320	0.120115
-88.847865	-14.209027	0.125120
-92.693908	-12.718718	0.130125
-96.337597	-12.405481	0.135130
-99.970053	-16.700014	0.140134
-103.798785	-12.743100	0.145139
-107.805717	-11.963488	0.150144
-111.360447	-12.189513	0.155149
-114.962949	-9.749340	0.160154
-118.667570	-20.350772	0.165158
-122.611980	-13.101830	0.170163
-126.343694	-6.832928	0.175168
-129.637315	-19.529327	0.180173
-133.952281	-17.748105	0.185178
-137.554311	-16.296660	0.190182
-141.673483	-21.565226	0.195187
-145.661023	-11.630298	0.200192
-149.170332	-14.154680	0.205197
-153.142368	-8.981147	0.210202
-156.439644	-23.681097	0.215206
-160.562905	-5.914349	0.220211
-164.202882	-14.460350	0.225216
-168.001537	-17.668613	0.230221
-171.823009	-10.639472	0.235226
-175.199039	-16.778724	0.240230
-179.233838	-4.731105	0.245235
-182.932521	-26.435977	0.250240
-186.064367	-13.775559	0.255245
-190.411043	-11.320592	0.260250
-194.067455	-16.962516	0.265254
-197.654886	-15.495967	0.270259
-201.809445	-14.465574	0.275264
-205.295170	-13.666483	0.280269
-209.268101	-10.648272	0.285274
-212.859870	-16.667890	0.290278
-216.723871	-13.001621	0.295283
-220.611487	-8.897943	0.300288
-224.105349	-9.698029	0.305293
-228.037394	-21.215400	0.310298
-231.448779	-18.091247	0.315302
-235.576283	-13.544011	0.320307
-239.231880	-14.805508	0.325312
-242.809157	-10.904280	0.330317
-246.994978	-14.178349	0.335322
-250.533747	-21.767444	0.340326
-254.524843	-3.807195	0.345331
-257.971959	-17.721462	0.350336
-261.652560	-15.640745	0.355341
-265.684303	-11.479302	0.360346
-269.078697	-15.452049	0.365350
-273.241882	-11.329534	0.370355
-276.973143	-4.056027	0.375360
-280.698511	-6.771218	0.380365
-284.376197	-6.900097	0.385370
-288.103891	-11.887142	0.390374
-292.131592	-17.491721	0.395379
-295.682572	-12.039844	0.400384
-299.612327	-15.140241	0.405389
-303.039607	-8.317319	0.410394
-307.016027	-15.029122	0.415398
-310.713098	-9.121845	0.420403
-314.659492	-5.897979	0.425408
-318.118439	-15.346204	0.430413
-322.261879	-9.366078	0.435418
-325.766299	-15.686450	0.440422
-329.253116	-17.939782	0.445427
-333.256853	-5.280337	0.450432
-336.755157	-30.200575	0.455437
-340.969847	-15.687770	0.460442
-344.568889	-22.240569	0.465446
-348.661582	-6.214525	0.470451
-352.168534	-24.732937	0.475456
-355.841378	-19.308827	0.480461
-359.853601	-7.217230	0.485466
-363.035951	-21.635611	0.490470
-367.299022	-23.038029	0.495475
-370.913261	-22.569818	0.500480
-374.851807	-12.530403	0.505485
-378.655633	-8.269555	0.510490
-381.894063	-17.737119	0.515494
-386.077317	-13.141310	0.520499
-389.901362	-20.549032	0.525504
-393.450275	-15.357527	0.530509
-397.521160	-6.777602	0.535514
-400.707880	-20.490380	0.540518
-404.825059	-13.571358	0.545523
-408.744995	-25.259063	0.550528
-412.365296	-16.279588	0.555533
-415.925290	-11.698096	0.560538
-419.553608	-23.280970	0.565542
-424.107065	-19.603629	0.570547
-427.786012	-4.255344	0.575552
-430.901283	-17.479629	0.580557
-434.979850	-12.574046	0.585562
-438.387449	-16.645355	0.590566
-442.589431	-17.554379	0.595571
-446.252773	-11.597100	0.600576
-449.973549	-12.593992	0.605581
-453.827883	-6.664544	0.610586
-457.227776	-10.647177	0.615590
-461.229628	-10.686173	0.620595
-464.750846	-20.012267	0.625600
-468.890700	-12.285328	0.630605
-472.663551	-7.940978	0.635610
-476.265299	-19.444432	0.640614
-480.082721	-13.240162	0.645619
-484.066512	-15.114297	0.650624
-487.360262	-19.817107	0.655629
-491.530863	-10.833205	0.660634
-495.034591	-20.948890	0.665638
-498.586194	-12.148985	0.670643
-502.549799	-10.737015	0.675648
-506.012598	-6.643969	0.680653
-510.174088	-12.985263	0.685658
-513.885516	-11.880038	0.690662
-517.832533	-4.333613	0.695667
-521.273783	-6.601825	0.700672
-525.161228	-5.887909	0.705677
-529.203185	-11.571795	0.710682
-532.585910	-17.748871	0.715686
-536.752216	-3.259237	0.720691
-540.261866	-22.060739	0.725696
-544.092136	-11.809717	0.730701
-547.849649	-6.567323	0.735706
-551.058337	-25.267075	0.740710
-555.522813	-7.604487	0.745715
-559.322022	-18.070239	0.750720
-562.972773	-11.455679	0.755725
-566.634118	-9.394921	0.760730
-570.229841	-13.778160	0.765734
-574.226990	-5.794738	0.770739
-577.758285	-12.209772	0.775744
-581.543601	-12.183814	0.780749
-585.210938	-13.666814	0.785754
-588.995468	-5.949129	0.790758
-592.772011	-10.159956	0.795763
-596.578512	-16.434807	0.800768
-600.228094	-9.970179	0.805773
-604.504758	-8.074397	0.810778
-607.782690	-18.583920	0.815782
-611.586715	-7.170123	0.820787
-615.347784	-10.610732	0.825792
-619.373791	-23.900535	0.830797
-623.310496	-13.591393	0.835802
-626.705062	-22.442335	0.840806
-630.637320	-12.424030	0.845811
-634.122251	-20.784318	0.850816
-638.071484	-11.553287	0.855821
-641.915473	-12.673684	0.860826
-645.311010	-20.518418	0.865830
-649.315184	-16.617777	0.870835
-653.249164	-10.251124	0.875840
-656.774751	-14.653318	0.880845
-660.800514	-14.109457	0.885850
-664.161269	-12.862923	0.890854
-668.024502	-9.254409	0.895859
-671.704774	-19.076696	0.900864
-675.590443	-15.295864	0.905869
-679.658824	-12.726804	0.910874
-683.039971	-15.212522	0.915878
-686.684817	-6.053701	0.920883
-690.585028	-18.587672	0.925888
-694.541451	-15.319015	0.930893
-698.299102	-15.320944	0.935898
-702.107216	-20.441111	0.940902
-705.800319	-8.097220	0.945907
-709.591112	-20.817362	0.950912
-713.414120	-6.514763	0.955917
-717.301148	-10.931642	0.960922
-720.631252	-11.153235	0.965926
-724.649225	-12.010744	0.970931
-728.186657	-11.305126	0.975936
-731.902888	-10.337557	0.980941
-735.915145	-10.774945	0.985946
-739.466594	-10.306749	0.990950
-743.395652	-8.370084	0.995955
-746.934639	-13.049099	1.000960
-750.700459	-10.506196	1.005965
-754.915723	-4.908076	1.010970
-758.045738	-6.779433	1.015974
-762.530080	-7.748410	1.020979
-765.888365	-11.021352	1.025984
-769.819796	-12.777223	1.030989
-773.748963	-21.436849	1.035994
-777.202122	-20.733589	1.040998
-781.009903	-20.307935	1.046003
-784.519462	-26.514817	1.051008
-788.411604	-17.420402	1.056013
-792.493431	-12.136839	1.061018
-795.992109	-20.934614	1.066022
-799.893537	-6.986759	1.071027
-803.685955	-15.387517	1.076032
-807.018628	-22.885685	1.081037
-811.141267	-19.459392	1.086042
-815.023611	-15.431304	1.091046
-818.887095	-5.668106	1.096051
-822.469273	-20.917533	1.101056
-825.695140	-17.623522	1.106061
-829.828176	-7.268481	1.111066
-833.436223	-16.975898	1.116070
-837.594665	-14.054731	1.121075
-841.243948	-20.663361	1.126080
-844.971905	-12.717810	1.131085
-848.610907	-29.703659	1.136090
-852.200763	-12.533602	1.141094
-856.255433	-19.668717	1.146099
-860.056540	-17.197268	1.151104
-863.839353	-22.772184	1.156109
-867.604101	-5.588331	1.161114
-871.120461	-19.755449	1.166118
-875.133622	-16.969398	1.171123
-878.578097	-22.768678	1.176128
-882.312439	-18.089257	1.181133
-886.308485	-16.326138	1.186138
-889.812055	-14.963420	1.191142
-893.701201	-12.783748	1.196147
-897.717165	-22.928850	1.201152
-901.299720	-29.314674	1.206157
-905.294886	-21.876632	1.211162
-908.956144	-21.970901	1.216166
-912.857378	-22.498270	1.221171
-916.418208	-13.642693	1.226176
-919.811379	-28.463306	1.231181
-923.959542	-18.509370	1.236186
-927.476168	-17.691671	1.241190
-931.673214	-7.576946	1.246195
-935.069251	-23.516636	1.251200
-938.793580	-8.319654	1.256205
-943.149276	-11.763990	1.261210
-946.623659	-13.247314	1.266214
-949.978959	-14.795403	1.271219
-954.144570	-7.333174	1.276224
-957.897858	-15.586972	1.281229
-961.350035	-17.218894	1.286234
-964.741254	-14.882201	1.291238
-969.104017	-7.464109	1.296243
-972.776223	-18.577036	1.301248
-976.706121	-21.354589	1.306253
-980.653440	-17.027284	1.311258
-984.237090	-20.585539	1.316262
-987.812450	-15.854114	1.321267
-991.559479	-16.230983	1.326272
-995.335938	-19.318450	1.331277
-999.305258	-7.543355	1.336282
-1002.571565	-26.152763	1.341286
-1006.863257	-2.703249	1.346291
-1010.826859	-11.207156	1.351296
-1013.916826	-16.613527	1.356301
-1017.788316	-9.778504	1.361306
-1021.618020	-12.526278	1.366310
-1025.633918	-14.099485	1.371315
-1029.274192	-18.738206	1.376320
-1033.121500	-18.616459	1.381325
-1036.546986	-7.644166	1.386330
-1039.969036	-13.904070	1.391334
-1044.178989	-16.231471	1.396339
-1047.943433	-10.772754	1.401344
-1051.757719	-24.524513	1.406349
-1055.885737	-10.476961	1.411354
-1059.565330	-19.898191	1.416358
-1063.465122	-17.912066	1.421363
-1066.957816	-23.067879	1.426368
-1070.290628	-18.502852	1.431373
-1074.455377	-2.613953	1.436378
-1078.100630	-24.305261	1.441382
-1081.929685	-14.274378	1.446387
-1085.810484	-9.594867	1.451392
-1089.224584	-12.464197	1.456397
-1093.603183	-21.891818	1.461402
-1096.631906	-25.754686	1.466406
-1100.497801	-11.340593	1.471411
-1104.642874	-14.003090	1.476416
-1108.156563	-24.510406	1.481421
-1112.103555	-10.720362	1.486426
-1115.785586	-24.865296	1.491430
-1119.890892	-12.830160	1.496435
-1123.322238	-16.116117	1.501440
-1126.913748	-18.561222	1.506445
-1130.786088	-16.057446	1.511450
-1134.426674	-24.065637	1.516454
-1138.567560	-8.252992	1.521459
-1142.375542	-12.741710	1.526464
-1145.547665	-13.935649	1.531469
-1149.622081	-21.682037	1.536474
-1153.154294	-20.423148	1.541478
-1156.663466	-23.529457	1.546483
-1161.180682	-16.250306	1.551488
-1164.765523	-23.489987	1.556493
-1168.586877	-7.711071	1.561498
-1172.175856	-26.590254	1.566502
-1176.168272	-25.978312	1.571507
-1179.681655	-21.715379	1.576512
-1183.255353	-24.365079	1.581517
-1187.320317	-17.811048	1.586522
-1190.848849	-18.069603	1.591526
-1195.070652	-12.917495	1.596531
-1198.357426	-21.854181	1.601536
-1201.847595	-25.075415	1.606541
-1206.022300	-19.019417	1.611546
-1209.769879	-21.959773	1.616550
-1213.428726	-6.066455	1.621555
-1217.369163	-21.440794	1.626560
-1220.639586	-21.445737	1.631565
-1225.103864	-24.014361	1.636570
-1228.544759	-12.055405	1.641574
-1232.492479	-15.662235	1.646579
-1236.331374	-13.879519	1.651584
-1239.964222	-14.323141	1.656589
-1243.611805	-12.930545	1.661594
-1247.115487	-14.389806	1.666598
-1251.070911	-12.711410	1.671603
-1255.286876	0.073315	1.676608
-1258.618269	-10.492898	1.681613
-1262.335774	-9.208922	1.686618
-1265.895910	-15.421149	1.691622
-1269.496840	-20.396912	1.696627
-1273.865008	-8.019855	1.701632
-1277.827100	-14.369570	1.706637
-1281.718540	-3.702388	1.711642
-1285.303570	-11.422783	1.716646
-1288.782726	-11.816814	1.721651
-1292.202085	-11.588102	1.726656
-1295.603984	-18.241888	1.731661
-1300.045439	3.363524	1.736666
-1303.912115	-1.787260	1.741670
-1307.674900	-13.605734	1.746675
-1311.426164	-6.281747	1.751680
-1315.097719	-17.570800	1.756685
-1318.758088	-11.647385	1.761690
-1322.335429	-13.597750	1.766694
-1326.594199	-14.819344	1.771699
-1330.204515	-10.165387	1.776704
-1333.753416	-12.214896	1.781709
-1337.832187	-12.438765	1.786714
-1341.533151	-20.455872	1.791718
-1345.478711	-19.419088	1.796723
-1349.018434	-4.361444	1.801728
-1352.366352	-13.955112	1.806733
-1356.263480	-9.308816	1.811738
-1360.021203	-19.082856	1.816742
-1364.221825	-15.406598	1.821747
-1367.857328	-18.244795	1.826752
-1371.567396	-9.881874	1.831757
-1375.506278	-11.433685	1.836762
-1378.915393	-10.936847	1.841766
-1382.475722	-8.099434	1.846771
-1386.647393	-8.295731	1.851776
-1390.022209	-18.044292	1.856781
-1394.040988	-15.333727	1.861786
-1397.978917	-17.235707	1.866790
-1401.722803	-10.849399	1.871795
-1405.539500	-11.654381	1.876800
-1408.778037	-7.510796	1.881805
-1413.055411	-5.115161	1.886810
-1416.431190	-28.071032	1.891814
-1420.578451	-10.126622	1.896819
-1424.189763	-9.480660	1.901824
-1427.791018	-16.635293	1.906829
-1431.789225	-17.745456	1.911834
-1435.316103	-13.535173	1.916838
-1439.378582	-10.282989	1.921843
-1443.084965	-13.929668	1.926848
-1446.572664	-18.863356	1.931853
-1450.911207	-7.894108	1.936858
-1454.367503	-17.623214	1.941862
-1458.076305	-13.278121	1.946867
-1461.563335	-18.577715	1.951872
-1465.258991	-11.992468	1.956877
-1469.296654	-16.945283	1.961882
-1472.623309	-13.752521	1.966886
-1476.900894	-1.596173	1.971891
-1480.624801	-14.552728	1.976896
-1484.404383	-12.090028	1.981901
-1488.298950	-0.116407	1.986906
-1491.647632	-16.110078	1.991910
-1495.532358	-10.211963	1.996915
-1499.885575	-12.426172	2.006912
-1500.869188	-14.292782	2.016909
-1497.727780	-14.952182	2.026906
-1495.121485	-21.653386	2.036902
-1492.991500	-15.507036	2.046899
-1490.951038	-18.118412	2.056896
-1489.652871	-9.167448	2.066893
-1487.512696	-20.743686	2.076890
-1485.687727	-15.986814	2.086886
-1483.406433	-15.471163	2.096883
-1481.635904	-20.401259	2.106880
-1479.551813	-12.346616	2.116877
-1478.141823	-14.814396	2.126874
-1476.102014	-12.417556	2.136870
-1473.975259	-16.656316	2.146867
-1472.109230	-9.457215	2.156864
-1470.321870	-14.143701	2.166861
-1468.206574	-13.009387	2.176858
-1466.677012	-17.967200	2.186854
-1464.766933	-15.416955	2.196851
-1462.489532	-25.409455	2.206848
-1460.952821	-21.664234	2.216845
-1459.088688	-16.146292	2.226842
-1457.192667	-18.830821	2.236838
-1455.187765	-11.586051	2.246835
-1452.911896	-20.201547	2.256832
-1451.642996	-17.292854	2.266829
-1449.632487	-12.333568	2.276826
-1447.456059	-25.562311	2.286822
-1445.589733	-23.055568	2.296819
-1443.820422	-24.096744	2.306816
-1441.975528	-18.177838	2.316813
-1440.160490	-20.416783	2.326810
-1438.286006	-26.457631	2.336806
-1436.236430	-17.205393	2.346803
-1434.672070	-17.201708	2.356800
-1432.710252	-13.344539	2.366797
-1430.667900	-14.866762	2.376794
-1428.932848	-20.755816	2.386790
-1427.084792	-20.502303	2.396787
-1425.072658	-23.465905	2.406784
-1423.044088	-17.273251	2.416781
-1421.408009	-16.365308	2.426778
-1419.346858	-16.933750	2.436774
-1417.431489	-18.849289	2.446771
-1415.869064	-11.904670	2.456768
-1413.703639	-20.917685	2.466765
-1411.919039	-11.627733	2.476762
-1410.278090	-8.154934	2.486758
-1408.284254	-10.915082	2.496755
-1406.169990	-16.307499	2.506752
-1404.336067	-12.341414	2.516749
-1402.558025	-14.774921	2.526746
-1400.536485	-15.586463	2.536742
-1398.818846	-9.025077	2.546739
-1396.610019	-10.450772	2.556736
-1394.954891	-12.356208	2.566733
-1393.367758	-4.752409	2.576730
-1390.918449	-11.996760	2.586726
-1389.339514	-11.330682	2.596723
-1387.752375	-6.054101	2.606720
-1385.694931	-9.868032	2.616717
-1383.844744	-11.853631	2.626714
-1381.918025	-16.759716	2.636710
-1379.703118	-13.571397	2.646707
-1378.043054	-16.535439	2.656704
-1376.380550	-9.796272	2.666701
-1374.132662	-9.038337	2.676698
-1372.502765	-9.924519	2.686694
-1370.745831	-11.269956	2.696691
-1368.433173	-8.850383	2.706688
-1366.827979	-13.507632	2.716685
-1365.097222	-12.737955	2.726682
-1363.232319	-13.461236	2.736678
-1360.903833	-10.505802	2.746675
-1359.272891	-15.138748	2.756672
-1357.718353	-12.132048	2.766669
-1355.536827	-8.744162	2.776666
-1353.753884	-11.456296	2.786662
-1351.723654	-9.630930	2.796659
-1349.930200	-13.601507	2.806656
-1347.941790	-15.160810	2.816653
-1346.240467	-14.359566	2.826650
-1344.090272	-20.313435	2.836646
-1342.390196	-17.541587	2.846643
-1340.746696	-9.228396	2.856640
-1338.681020	-12.167342	2.866637
-1336.773372	-16.276180	2.876634
-1334.751586	-17.034022	2.886630
-1333.116891	-11.026114	2.896627
-1331.103032	-13.053658	2.906624
-1329.113597	-14.488380	2.916621
-1327.608662	-9.894871	2.926618
-1325.544899	-5.954454	2.936614
-1323.637547	-8.089674	2.946611
-1321.890060	-5.003311	2.956608
-1319.578653	-13.880153	2.966605
-1317.839807	-15.847879	2.976602
-1316.279506	-9.835943	2.986598
-1314.346727	-10.164285	2.996595
-1312.450630	-16.866883	3.006592
-1310.379156	-9.634209	3.016589
-1308.839980	-11.590495	3.026586
-1306.807033	-5.463159	3.036582
-1304.649190	-8.588923	3.046579
-1302.946606	-14.867408	3.056576
-1301.108195	-6.849048	3.066573
-1298.965529	-12.359597	3.076570
-1297.291214	-19.457712	3.086566
-1295.702157	-5.554538	3.096563
-1293.767204	-11.117098	3.106560
-1291.769778	-10.371098	3.116557
-1289.762653	-14.543185	3.126554
-1287.942338	-16.501824	3.136550
-1286.055642	-15.641788	3.146547
-1284.392198	-15.731222	3.156544
-1282.235059	-11.114175	3.166541
-1280.393715	-9.501658	3.176538
-1278.639458	-7.227874	3.186534
-1276.568120	-14.735285	3.196531
-1274.771592	-19.269946	3.206528
-1272.920911	-12.178733	3.216525
-1271.154686	-15.717025	3.226522
-1269.301727	-14.425286	3.236518
-1267.424198	-10.188187	3.246515
-1265.442296	-14.460422	3.256512
-1263.356660	-11.674430	3.266509
-1261.780477	-4.352969	3.276506
-1259.863942	-11.609820	3.286502
-1257.839357	-12.260682	3.296499
-1256.362298	-13.971745	3.306496
-1254.323662	-11.500309	3.316493
-1252.220742	-4.209454	3.326490
-1250.151190	-13.203836	3.336486
-1248.353944	-12.163675	3.346483
-1246.433131	-10.990138	3.356480
-1244.689365	-13.981693	3.366477
-1243.258322	-13.850761	3.376474
-1241.169189	-14.578250	3.386470
-1239.244425	-18.004529	3.396467
-1237.096836	-19.614472	3.406464
-1235.371994	-18.063798	3.416461
-1233.618877	-16.740265	3.426458
-1231.669285	-17.462783	3.436454
-1229.794099	-14.887807	3.446451
-1228.043094	-16.328498	3.456448
-1225.997535	-21.202955	3.466445
-1224.121808	-14.450423	3.476442
-1222.226002	-18.612535	3.486438
-1220.493206	-14.199089	3.496435
-1218.512417	-14.427671	3.506432
-1216.788504	-14.724089	3.516429
-1214.819306	-15.550777	3.526426
-1213.031043	-13.503423	3.536422
-1211.002809	-12.435460	3.546419
-1209.117038	-10.822100	3.556416
-1207.074424	-10.760584	3.566413
-1205.243340	-13.802396	3.576410
-1203.677424	-10.481638	3.586406
-1201.672111	-7.305390	3.596403
-1199.613894	-13.662815	3.606400
-1197.933836	-14.039039	3.616397
-1195.815580	-13.923304	3.626394
-1194.371557	-14.347016	3.636390
-1192.379000	-8.650452	3.646387
-1190.341663	-8.692281	3.656384
-1188.571644	-10.105988	3.666381
-1186.869437	-17.039558	3.676378
-1184.624893	-10.837023	3.686374
-1182.686280	-18.092609	3.696371
-1181.030614	-9.152853	3.706368
-1179.140976	-7.836911	3.716365
-1177.273933	-5.102700	3.726362
-1175.268575	-9.863325	3.736358
-1173.357028	-19.702309	3.746355
-1171.605970	-15.143334	3.756352
-1169.578823	-17.483900	3.766349
-1168.011900	-16.220522	3.776346
-1166.213520	-12.651157	3.786342
-1164.183754	-13.957991	3.796339
-1162.236824	-15.073160	3.806336
-1160.338827	-17.467261	3.816333
-1158.066675	-7.326723	3.826330
-1156.594419	-18.213243	3.836326
-1155.090247	-14.132618	3.846323
-1152.692097	-14.598433	3.856320
-1150.735289	-9.712377	3.866317
-1149.057532	-10.465544	3.876314
-1147.314753	-7.446181	3.886310
-1145.433002	-3.138601	3.896307
-1143.661405	-15.708697	3.906304
-1141.714247	-11.811031	3.916301
-1139.499005	-12.315461	3.926298
-1138.074178	-11.877172	3.936294
-1135.873641	-4.611292	3.946291
-1134.119292	-10.320088	3.956288
-1132.095700	-11.215405	3.966285
-1130.529650	-9.127699	3.976282
-1128.275153	-6.714364	3.986278
-1126.423648	-13.363904	3.996275
-1124.533140	-10.884442	4.006272
-1122.795218	-12.160341	4.016269
-1121.031825	-11.810938	4.026266
-1119.210669	-8.840405	4.036262
-1117.320456	-9.401760	4.046259
-1115.426565	-4.532447	4.056256
-1113.303597	-6.981448	4.066253
-1111.355849	-9.342421	4.076250
-1109.849352	-10.387091	4.086246
-1107.894386	-8.989967	4.096243
-1105.904199	-8.548944	4.106240
-1103.822730	-14.850014	4.116237
-1102.217796	-7.812490	4.126234
-1100.438597	-20.008004	4.136230
-1098.429983	-11.991432	4.146227
-1096.511374	-13.689349	4.156224
-1094.239493	-11.103509	4.166221
-1092.960118	-12.361296	4.176218
-1091.317271	-5.314038	4.186214
-1089.233969	-12.804267	4.196211
-1087.024574	-17.644820	4.206208
-1084.940138	-8.476747	4.216205
-1083.454951	-13.285136	4.226202
-1081.533211	-9.634387	4.236198
-1079.743568	-15.284057	4.246195
-1077.899737	-11.647685	4.256192
-1075.960586	-12.322617	4.266189
-1074.031269	-12.667573	4.276186
-1071.865976	-14.834376	4.286182
-1070.234763	-10.444032	4.296179
-1068.627235	-20.076429	4.306176
-1066.637818	-17.514851	4.316173
-1064.645999	-12.454330	4.326170
-1062.810292	-14.442100	4.336166
-1061.049957	-9.385600	4.346163
-1059.167311	-14.194392	4.356160
-1057.024083	-6.900320	4.366157
-1055.085061	-12.978052	4.376154
-1053.219801	-13.235381	4.386150
-1051.698501	-10.057370	4.396147
-1049.612446	-13.405093	4.406144
-1047.576998	-16.774718	4.416141
-1045.894014	-13.587828	4.426138
-1044.018811	-10.426943	4.436134
-1042.178567	-17.608273	4.446131
-1040.586021	-14.957935	4.456128
-1038.541201	-21.339924	4.466125
-1036.477109	-15.444672	4.476122
-1034.499954	-11.801168	4.486118
-1032.552183	-18.418669	4.496115
-1030.445945	-17.745106	4.506112
-1029.342023	-11.704176	4.516109
-1027.358970	-14.388077	4.526106
-1025.094446	-13.360898	4.536102
-1023.311506	-17.373762	4.546099
-1021.384462	-19.131386	4.556096
-1019.513680	-14.804580	4.566093
-1017.934984	-19.975231	4.576090
-1016.090605	-12.123356	4.586086
-1013.852237	-7.713234	4.596083
-1011.929413	-16.259249	4.606080
-1010.204892	-16.779809	4.616077
-1008.442945	-11.818256	4.626074
-1006.557662	-12.105591	4.636070
-1004.566239	-6.205000	4.646067
-1002.646965	-15.249359	4.656064
-1001.054556	-16.498741	4.666061
-998.948745	-11.933204	4.676058
-996.880345	-10.350453	4.686054
-995.181527	-19.144825	4.696051
-993.412835	-17.986221	4.706048
-991.480556	-13.566600	4.716045
-989.795790	-11.930388	4.726042
-987.936578	-12.511943	4.736038
-985.730635	-8.180287	4.746035
-983.922057	-14.838648	4.756032
-982.253945	-12.190878	4.766029
-980.177456	-11.474619	4.776026
-978.339675	-8.623465	4.786022
-976.362819	-21.411003	4.796019
-974.399574	-18.406237	4.806016
-972.700319	-10.335338	4.816013
-970.879025	-17.688840	4.826010
-969.093297	-8.905492	4.836006
-966.677795	-21.687380	4.846003
-965.249756	-15.797714	4.856000
-963.408976	-23.252213	4.865997
-961.344809	-22.897103	4.875994
-959.618329	-14.353735	4.885990
-957.626908	-23.160135	4.895987
-955.959599	-23.641509	4.905984
-953.899894	-21.214222	4.915981
-952.001197	-16.192391	4.925978
-950.316893	-15.486022	4.935974
-948.231980	-14.534253	4.945971
-946.377848	-11.358865	4.955968
-944.450478	-19.124023	4.965965
-942.969548	-7.634702	4.975962
-940.898022	-14.257714	4.985958
-939.091548	-8.210656	4.995955
-936.851107	-7.285323	5.005952
-935.316025	-6.981373	5.015949
-933.342813	-13.220786	5.025946
-931.453166	-3.768795	5.035942
-929.460199	-8.141999	5.045939
-927.689223	-2.935520	5.055936
-925.607318	-9.048632	5.065933
-924.002906	-5.045447	5.075930
-922.089526	-9.385395	5.085926
-920.193784	-5.250377	5.095923
-918.214065	-8.792554	5.105920
-916.539090	-6.676328	5.115917
-914.507815	-11.412466	5.125914
-912.798361	-12.677345	5.135910
-910.761790	0.267290	5.145907
-908.665949	-9.460462	5.155904
-907.107346	-11.339076	5.165901
-904.943228	-7.333791	5.175898
-903.382722	-7.147564	5.185894
-901.296131	-6.331801	5.195891
-899.437748	-10.980289	5.205888
-897.838514	-8.381441	5.215885
-895.786677	-10.878874	5.225882
-893.816494	-12.805915	5.235878
-891.869945	-4.493446	5.245875
-890.157778	-13.059377	5.255872
-888.370550	-12.115222	5.265869
-886.741888	-1.434163	5.275866
-884.737392	-8.780585	5.285862
-882.456074	-6.098151	5.295859
-880.529130	-15.389950	5.305856
-878.805385	-14.426166	5.315853
-876.899779	-5.941359	5.325850
-875.227323	-1.609561	5.335846
-873.515278	-7.208791	5.345843
-871.331270	-11.718273	5.355840
-869.262432	-11.256466	5.365837
-867.591106	-9.938522	5.375834
-865.541016	-12.699320	5.385830
-863.960070	-8.575506	5.395827
-862.119044	-15.370014	5.405824
-859.926838	-7.598866	5.415821
-858.435894	-17.079882	5.425818
-856.559055	-12.125521	5.435814
-854.491181	-1.292030	5.445811
-852.387435	-9.372673	5.455808
-850.782976	-6.457276	5.465805
-848.820682	-14.884753	5.475802
-846.883063	-10.282712	5.485798
-845.170891	-14.268348	5.495795
-843.257235	-6.222141	5.505792
-841.396794	-5.365437	5.515789
-839.312244	-10.875777	5.525786
-837.593567	-7.476552	5.535782
-835.964936	-9.168958	5.545779
-833.857961	-13.130859	5.555776
-832.118402	-7.085645	5.565773
-830.188293	-9.020438	5.575770
-828.282130	-11.241911	5.585766
-826.292894	-14.801323	5.595763
-824.348546	-11.326063	5.605760
-822.745590	-9.250358	5.615757
-820.622571	-13.996348	5.625754
-818.853610	-11.944018	5.635750
-817.064347	-12.541098	5.645747
-814.958947	-16.078018	5.655744
-813.012734	-16.381253	5.665741
-811.399091	-15.633490	5.675738
-809.523796	-18.257359	5.685734
-807.746820	-14.685863	5.695731
-805.680741	-16.999191	5.705728
-803.729251	-17.756393	5.715725
-801.952909	-22.865349	5.725722
-800.064476	-25.650774	5.735718
-798.323921	-20.404599	5.745715
-796.374375	-21.706191	5.755712
-794.309449	-17.107086	5.765709
-792.482501	-26.663870	5.775706
-790.587992	-22.571179	5.785702
-788.885465	-21.768137	5.795699
-786.970359	-17.058243	5.805696
-785.265687	-27.978557	5.815693
-783.284758	-26.468473	5.825690
-781.170901	-15.102299	5.835686
-779.382504	-22.122006	5.845683
-777.683841	-25.003392	5.855680
-775.634385	-25.801491	5.865677
-773.680331	-26.075948	5.875674
-771.730833	-26.725444	5.885670
-770.122420	-25.796827	5.895667
-768.275154	-21.652359	5.905664
-766.368605	-23.037049	5.915661
-764.396192	-22.824987	5.925658
-762.317330	-23.893022	5.935654
-760.970530	-24.473026	5.945651
-758.599230	-25.279918	5.955648
-757.085964	-24.028209	5.965645
-755.221027	-21.943805	5.975642
-753.050595	-19.868751	5.985638
-751.284919	-24.832290	5.995635
-749.591042	-25.993515	6.005632
-747.508809	-19.586184	6.015629
-745.549617	-12.328705	6.025626
-743.755352	-22.589143	6.035622
-741.973483	-16.473258	6.045619
-740.042858	-13.431497	6.055616
-738.173539	-20.047290	6.065613
-736.103091	-22.365993	6.075610
-734.377465	-13.920190	6.085606
-732.610730	-20.091715	6.095603
-730.704905	-19.562685	6.105600
-728.942940	-14.765112	6.115597
-727.137296	-19.924486	6.125594
-725.106988	-19.780061	6.135590
-723.139921	-21.482265	6.145587
-721.106940	-21.627195	6.155584
-719.228577	-24.420422	6.165581
-717.738058	-20.967281	6.175578
-715.878702	-14.429569	6.185574
-713.718710	-15.054237	6.195571
-711.311120	-20.636615	6.205568
-710.164475	-17.635331	6.215565
-708.382251	-23.551958	6.225562
-705.936253	-13.877637	6.235558
-704.474472	-13.066062	6.245555
-702.782942	-19.492376	6.255552
-700.760743	-16.241018	6.265549
-698.468386	-15.446903	6.275546
-696.868760	-13.226902	6.285542
-695.050275	-9.049350	6.295539
-693.149611	-18.166298	6.305536
-691.119374	-8.532884	6.315533
-689.235590	-15.199900	6.325530
-687.474714	-17.647507	6.335526
-685.852736	-14.872154	6.345523
-683.494095	-12.686588	6.355520
-681.750836	-18.866958	6.365517
-680.025668	-14.706062	6.375514
-678.443677	-17.180339	6.385510
-676.272879	-11.213380	6.395507
-674.418542	-13.252777	6.405504
-672.394287	-18.537038	6.415501
-670.497131	-23.047873	6.425498
-668.893807	-19.783240	6.435494
-666.970457	-19.909027	6.445491
-665.107915	-23.174922	6.455488
-663.039974	-19.881895	6.465485
-660.928893	-18.353029	6.475482
-659.323854	-12.614588	6.485478
-657.550104	-14.383741	6.495475
-655.686114	-15.966796	6.505472
-653.436247	-20.439242	6.515469
-652.080531	-22.991026	6.525466
-650.026426	-21.633038	6.535462
-648.034419	-17.797367	6.545459
-646.327344	-20.970518	6.555456
-644.507427	-15.414811	6.565453
-642.279386	-18.293847	6.575450
-640.506057	-15.397388	6.585446
-638.625264	-16.392621	6.595443
-636.994642	-11.095594	6.605440
-635.001406	-16.145936	6.615437
-632.961421	-12.529483	6.625434
-631.181288	-14.853818	6.635430
-629.518541	-12.858579	6.645427
-627.379747	-14.578670	6.655424
-625.850013	-16.335656	6.665421
-623.735985	-13.441512	6.675418
-621.861144	-22.154830	6.685414
-619.925726	-13.811920	6.695411
-618.039154	-13.320773	6.705408
-616.100845	-16.603473	6.715405
-614.214690	-16.615913	6.725402
-612.601435	-15.091151	6.735398
-610.600884	-8.639058	6.745395
-608.726580	-15.021885	6.755392
-606.612026	-18.605877	6.765389
-604.963279	-21.805995	6.775386
-603.075375	-19.327263	6.785382
-601.122600	-13.617490	6.795379
-599.520475	-12.092519	6.805376
-597.349414	-13.028307	6.815373
-595.499333	-14.204906	6.825370
-593.773818	-12.454919	6.835366
-591.806118	-21.803544	6.845363
-589.777614	-14.410162	6.855360
-588.042865	-25.309904	6.865357
-586.062741	-16.666228	6.875354
-584.361039	-18.992208	6.885350
-582.604562	-17.458728	6.895347
-580.576754	-18.568974	6.905344
-578.715630	-18.986312	6.915341
-576.624568	-20.458745	6.925338
-574.785380	-16.901739	6.935334
-573.162325	-16.013218	6.945331
-571.565910	-19.978597	6.955328
-569.290646	-22.759326	6.965325
-567.271794	-18.539473	6.975322
-565.473948	-16.955748	6.985318
-563.675150	-20.443478	6.995315
-561.708278	-20.495610	7.005312
-559.856018	-14.401870	7.015309
-558.239394	-23.048636	7.025306
-556.105662	-15.278896	7.035302
-554.181783	-17.281943	7.045299
-552.364572	-16.626515	7.055296
-550.646006	-21.805011	7.065293
-548.395078	-15.277600	7.075290
-546.705552	-20.408827	7.085286
-545.155046	-17.917205	7.095283
-543.246500	-9.892018	7.105280
-541.249225	-15.163973	7.115277
-539.403671	-11.912675	7.125274
-537.394858	-13.779284	7.135270
-535.505910	-13.804738	7.145267
-533.537911	-11.234536	7.155264
-531.690424	-18.081946	7.165261
-529.704928	-16.242392	7.175258
-528.025275	-18.272722	7.185254
-526.140032	-18.589667	7.195251
-524.354181	-12.628966	7.205248
-522.238206	-17.461994	7.215245
-520.323824	-12.863852	7.225242
-518.824771	-21.234463	7.235238
-517.009616	-13.026978	7.245235
-515.000976	-11.650556	7.255232
-512.888931	-16.411901	7.265229
-510.966154	-10.861457	7.275226
-509.124183	-19.866276	7.285222
-507.481328	-11.001297	7.295219
-505.739110	-13.169494	7.305216
-503.708548	-9.254593	7.315213
-501.498807	-12.477930	7.325210
-499.602689	-11.547709	7.335206
-498.043460	-10.388429	7.345203
-496.470392	-9.365561	7.355200
-494.044051	-15.088091	7.365197
-492.366125	-10.117440	7.375194
-490.665564	-7.592905	7.385190
-488.789458	-7.913098	7.395187
-486.546984	-10.167490	7.405184
-484.721381	-14.643078	7.415181
-482.994296	-12.991149	7.425178
-481.031495	-11.103720	7.435174
-479.085774	-8.992520	7.445171
-477.320276	-6.682019	7.455168
-475.571985	-13.755116	7.465165
-473.283289	-17.155238	7.475162
-471.931181	-16.223376	7.485158
-470.026919	-14.727621	7.495155
-467.704579	-18.770971	7.505152
-466.139006	-8.273703	7.515149
-464.122521	-18.790493	7.525146
-462.419771	-14.115876	7.535142
-460.458846	-19.921933	7.545139
-458.418271	-4.378677	7.555136
-456.734307	-11.517276	7.565133
-454.631478	-11.870490	7.575130
-452.979902	-17.598723	7.585126
-451.188768	-16.861688	7.595123
-449.273396	-9.694830	7.605120
-447.199641	-14.773672	7.615117
-445.346613	-19.555173	7.625114
-443.423569	-14.086816	7.635110
-441.549998	-13.186105	7.645107
-439.870707	-16.580457	7.655104
-438.193987	-7.476105	7.665101
-436.376175	-11.344131	7.675098
-434.063096	-11.446705	7.685094
-432.334727	-14.373650	7.695091
-430.403540	-9.926527	7.705088
-428.544776	-9.563413	7.715085
-426.541619	-11.233248	7.725082
-424.873288	-14.862670	7.735078
-422.809687	-8.856240	7.745075
-421.320002	-11.096153	7.755072
-419.315026	-16.574495	7.765069
-417.251632	-16.239310	7.775066
-415.313174	-17.565665	7.785062
-413.717177	-13.005009	7.795059
-411.842259	-17.158436	7.805056
-409.899047	-10.870680	7.815053
-407.625813	-24.570363	7.825050
-406.067927	-18.448439	7.835046
-404.311173	-17.276427	7.845043
-402.252705	-17.682509	7.855040
-400.287269	-11.783537	7.865037
-398.498300	-15.217478	7.875034
-396.632814	-14.539639	7.885030
-394.967874	-13.665576	7.895027
-392.950617	-13.859818	7.905024
-391.037247	-15.804220	7.915021
-388.887470	-13.397122	7.925018
-387.310014	-21.882807	7.935014
-385.823686	-17.186209	7.945011
-383.725109	-13.002602	7.955008
-381.565174	-7.428334	7.965005
-379.631742	-8.894378	7.975002
-377.820110	-8.261607	7.984998
-375.945022	-4.527020	7.994995
-373.998820	-9.290192	8.004992
-372.741339	-11.595629	8.014989
-370.492905	-12.445676	8.024986
-368.044319	-10.278886	8.034982
-366.736226	-12.012956	8.044979
-364.556769	-9.860034	8.054976
-362.740387	-7.527571	8.064973
-361.170537	-8.902397	8.074970
-359.169736	-4.178971	8.084966
-357.472919	-4.317287	8.094963
-355.348821	-9.921962	8.104960
-353.409310	-19.998511	8.114957
-351.741112	-14.634644	8.124954
-349.486712	-21.515311	8.134950
-348.047180	-12.628800	8.144947
-346.172639	-17.205254	8.154944
-344.096462	-20.975518	8.164941
-342.118255	-15.918491	8.174938
-340.171299	-21.046473	8.184934
-338.568649	-19.017749	8.194931
-336.722949	-5.415261	8.204928
-334.901190	-17.981819	8.214925
-333.102228	-21.698346	8.224922
-330.880979	-20.739373	8.234918
-329.084478	-18.190565	8.244915
-327.385477	-14.907805	8.254912
-325.320418	-12.400286	8.264909
-323.342249	-11.746693	8.274906
-321.658648	-10.747670	8.284902
-319.739710	-9.715163	8.294899
-317.721567	-14.357151	8.304896
-316.083670	-13.843434	8.314893
-314.096183	-9.937276	8.324890
-312.236208	-16.202347	8.334886
-310.250105	-16.236817	8.344883
-308.513518	-19.281825	8.354880
-306.834005	-16.695377	8.364877
-304.846499	-13.826531	8.374874
-302.807619	-18.896531	8.384870
-300.949135	-16.528112	8.394867
-299.045100	-18.182020	8.404864
-297.171021	-13.623042	8.414861
-295.281536	-21.334315	8.424858
-293.346069	-21.461736	8.434854
-291.538103	-18.330548	8.444851
-289.913865	-17.449914	8.454848
-287.706218	-20.486419	8.464845
-286.113323	-17.393525	8.474842
-284.127728	-18.496785	8.484838
-282.181987	-16.776983	8.494835
-280.279282	-13.544072	8.504832
-278.585004	-16.833346	8.514829
-276.519993	-22.869024	8.524826
-274.657910	-15.570358	8.534822
-272.967084	-13.519349	8.544819
-270.969357	-14.310340	8.554816
-269.067824	-23.758692	8.564813
-267.018562	-16.733042	8.574810
-265.387757	-16.753394	8.584807
-263.472539	-11.261527	8.594803
-261.590762	-16.353785	8.604800
-259.672638	-11.501820	8.614797
-257.827558	-17.300288	8.624794
-256.075387	-24.495429	8.634791
-253.726316	-16.581351	8.644787
-252.211160	-20.112004	8.654784
-250.146742	-20.930990	8.664781
-248.604321	-19.121527	8.674778
-246.528165	-19.246103	8.684775
-244.908780	-18.734119	8.694771
-242.944760	-16.837212	8.704768
-240.952501	-12.315995	8.714765
-238.840113	-19.333368	8.724762
-237.273847	-20.341244	8.734759
-235.421298	-17.352910	8.744755
-233.135318	-23.629074	8.754752
-231.786606	-14.934820	8.764749
-229.701066	-19.058572	8.774746
-227.440493	-19.792009	8.784743
-225.752492	-21.103503	8.794739
-223.887752	-25.299373	8.804736
-222.002896	-29.275831	8.814733
-220.433221	-29.006937	8.824730
-218.581004	-21.469822	8.834727
-216.488162	-27.749880	8.844723
-214.673038	-30.147389	8.854720
-212.759569	-20.861186	8.864717
-210.807305	-28.615572	8.874714
-209.119284	-29.627072	8.884711
-207.384145	-25.960014	8.894707
-205.293515	-27.386272	8.904704
-203.217850	-23.258843	8.914701
-201.640347	-24.693205	8.924698
-199.709145	-29.715937	8.934695
-197.546796	-24.329770	8.944691
-196.158258	-26.351310	8.954688
-194.022125	-25.307577	8.964685
-192.294891	-25.300639	8.974682
-190.164013	-29.690525	8.984679
-188.335640	-28.296111	8.994675
-186.682087	-28.154259	9.004672
-184.603900	-28.620142	9.014669
-182.579405	-23.734566	9.024666
-181.003229	-27.683840	9.034663
-179.069412	-30.068686	9.044659
-177.267060	-22.130440	9.054656
-175.156390	-24.968222	9.064653
-173.244342	-24.905502	9.074650
-171.580494	-22.895903	9.084647
-169.612420	-24.222052	9.094643
-167.709838	-25.640375	9.104640
-166.157290	-22.957781	9.114637
-164.376436	-28.791718	9.124634
-161.831888	-28.665716	9.134631
-160.286332	-27.551398	9.144627
-158.475580	-27.035157	9.154624
-156.230817	-30.142201	9.164621
-154.581784	-29.892242	9.174618
-152.797945	-30.192714	9.184615
-150.910602	-26.551478	9.194611
-149.106143	-26.116327	9.204608
-147.038218	-26.068987	9.214605
-145.066252	-24.136953	9.224602
-143.711505	-31.775421	9.234599
-141.623041	-20.996627	9.244595
-139.438469	-20.811585	9.254592
-137.712487	-20.254961	9.264589
-135.821639	-20.362505	9.274586
-134.048832	-21.962191	9.284583
-132.126805	-16.464985	9.294579
-130.274094	-11.431954	9.304576
-128.567414	-7.215580	9.314573
-126.246338	-13.490938	9.324570
-124.361181	-8.403082	9.334567
-122.996296	-12.667542	9.344563
-120.934819	-12.034968	9.354560
-119.109754	-7.824844	9.364557
-117.168172	-10.755595	9.374554
-115.067136	-8.556772	9.384551
-113.231848	-8.664907	9.394547
-111.858313	-8.674106	9.404544
-109.777433	-5.261068	9.414541
-107.368596	-16.353336	9.424538
-105.878471	-16.180617	9.434535
-103.809582	-12.865132	9.444531
-102.101883	-15.799605	9.454528
-100.509507	-12.123894	9.464525
-98.449784	-10.745794	9.474522
-96.589445	-16.540268	9.484519
-94.465659	-17.618056	9.494515
-92.578148	-20.304908	9.504512
-90.700933	-17.171979	9.514509
-89.091224	-22.361224	9.524506
-87.344877	-17.271720	9.534503
-85.150283	-13.696813	9.544499
-83.179890	-19.000438	9.554496
-81.611092	-18.530797	9.564493
-79.661770	-15.152007	9.574490
-77.758345	-23.211124	9.584487
-75.794709	-21.789256	9.594483
-73.843923	-22.951526	9.604480
-72.156941	-14.770584	9.614477
-70.277089	-17.639347	9.624474
-68.112474	-18.540476	9.634471
-66.432068	-15.014569	9.644467
-64.565554	-17.192811	9.654464
-62.833385	-17.131307	9.664461
-61.081835	-13.250447	9.674458
-58.942644	-14.687486	9.684455
-57.223363	-23.225610	9.694451
-55.106814	-19.729800	9.704448
-53.263056	-14.196356	9.714445
-51.299095	-16.388555	9.724442
-49.475026	-20.233619	9.734439
-47.897625	-22.357834	9.744435
-45.508964	-15.880306	9.754432
-43.927699	-13.961646	9.764429
-42.123447	-22.008077	9.774426
-39.946000	-18.308820	9.784423
-38.571426	-19.944381	9.794419
-36.493209	-24.221535	9.804416
-34.513913	-25.933032	9.814413
-32.640465	-18.274413	9.824410
-30.827812	-16.705271	9.834407
-29.074596	-14.694036	9.844403
-27.166402	-14.120611	9.854400
-24.891071	-13.432072	9.864397
-23.092020	-19.338290	9.874394
-21.453202	-20.693902	9.884391
-19.924464	-22.262469	9.894387
-17.766048	-17.412316	9.904384
-15.727009	-17.095005	9.914381
-13.909735	-13.573523	9.924378
-12.079778	-10.807184	9.934375
-10.077397	-17.453162	9.944371
-8.371165	-10.157826	9.954368
-6.401502	-5.222290	9.964365
-5.234652	8.701944	9.974362
-3.865572	42.969346	9.984359
-2.635746	97.857154	9.994355
-1.285708	167.160220	10.004352
0.000000	231.940393	10.009357
0.300240	274.911408	10.014362
1.031211	303.199245	10.019367
1.582579	352.122608	10.024371
2.316901	371.663023	10.029376
2.487304	402.806342	10.034381
2.948350	416.836571	10.039386
3.066189	427.023455	10.044391
3.153992	437.327097	10.049395
3.474735	454.151935	10.054400
3.309333	469.010664	10.059405
3.554987	472.016466	10.064410
3.911262	470.586133	10.069415
3.559435	482.052725	10.074419
3.954085	486.272637	10.079424
4.162302	507.972362	10.084429
4.137342	505.104769	10.089434
4.384581	509.393931	10.094439
4.252989	512.281722	10.099443
4.523997	503.866660	10.104448
4.577929	512.737617	10.109453
4.443144	498.379254	10.114458
4.277003	494.725228	10.119463
4.313522	504.215528	10.124467
4.765977	503.055272	10.129472
4.539993	498.057802	10.134477
4.584179	498.386615	10.139482
4.587509	505.409617	10.144487
4.588006	520.404359	10.149491
4.970599	511.000117	10.154496
4.803065	527.858768	10.159501
4.557086	528.620207	10.164506
4.683394	532.113400	10.169511
4.631860	530.249804	10.174515
4.758230	541.009404	10.179520
5.090384	541.777976	10.184525
5.149730	532.631854	10.189530
5.233438	536.874569	10.194535
5.180424	540.934095	10.199539
5.258106	537.130783	10.204544
5.478223	535.895623	10.209549
4.994183	541.569272	10.214554
5.334472	550.869229	10.219559
5.143030	549.970941	10.224563
5.018610	553.031056	10.229568
5.019048	559.529433	10.234573
5.498607	551.656653	10.239578
5.327667	555.272956	10.244583
5.201575	562.092706	10.249587
5.344339	543.105936	10.254592
5.526656	570.926737	10.259597
5.632875	576.641868	10.264602
5.898476	586.237606	10.269607
5.843596	595.578545	10.274611
5.904913	588.352761	10.279616
6.202113	594.240860	10.284621
6.006390	590.009645	10.289626
5.807189	567.740626	10.294631
5.578242	590.539930	10.299635
5.817757	589.360016	10.304640
5.730340	591.564279	10.309645
5.640262	608.841169	10.314650
6.241330	603.350631	10.319655
6.151793	607.539000	10.324659
6.274556	604.135327	10.329664
5.979406	611.918756	10.334669
6.218541	605.180256	10.339674
6.235565	608.630976	10.344679
6.370705	612.239472	10.349683
6.460668	613.139717	10.354688
6.695000	621.042121	10.359693
6.581012	634.058857	10.364698
6.759643	619.620423	10.369703
6.711337	621.452606	10.374707
6.849294	607.298209	10.379712
6.656384	622.114174	10.384717
6.525977	619.521993	10.389722
6.748949	625.007213	10.394727
6.783825	650.483146	10.399731
7.012533	641.144366	10.404736
6.941158	649.712124	10.409741
6.900367	654.879887	10.414746
7.087666	642.031166	10.419751
7.051162	646.838703	10.424755
7.112582	656.634209	10.429760
7.334407	647.909947	10.434765
7.288954	646.646174	10.439770
7.679198	660.014586	10.444775
7.296769	661.395450	10.449779
7.089641	660.947503	10.454784
7.541628	654.376877	10.459789
7.242206	656.359502	10.464794
7.450101	658.925096	10.469799
7.329734	658.296157	10.474803
7.610749	655.586308	10.479808
7.653893	653.813249	10.484813
7.286171	657.449925	10.489818
7.402864	662.018570	10.494823
7.203073	661.495338	10.499827
7.555001	655.625056	10.504832
7.828928	667.334179	10.509837
8.027623	670.345936	10.514842
7.721498	671.440245	10.519847
7.833481	675.785722	10.524851
8.113957	688.615013	10.529856
8.150677	694.123660	10.534861
8.145956	694.941241	10.539866
8.454987	687.817822	10.544871
8.148614	685.606928	10.549875
8.164853	698.834759	10.554880
8.341875	700.332972	10.559885
8.266918	704.511159	10.564890
8.435218	697.140527	10.569895
8.353375	706.845378	10.574899
8.946696	689.801871	10.579904
8.690733	682.368031	10.584909
8.199003	680.044778	10.589914
8.680232	684.383402	10.594919
8.310504	694.734973	10.599923
8.391240	693.668685	10.604928
8.837210	706.036363	10.609933
8.967647	702.051132	10.614938
8.792285	697.636866	10.619943
8.859040	709.166181	10.624947
8.892605	712.092323	10.629952
8.853857	706.803145	10.634957
8.808270	715.557637	10.639962
8.879045	706.273967	10.644967
8.983581	705.952925	10.649971
8.874032	706.107570	10.654976
9.062449	712.424647	10.659981
8.926679	705.685974	10.664986
9.020013	707.617000	10.669991
9.109670	720.025752	10.674995
9.046137	717.936967	10.680000
9.035709	720.040661	10.685005
9.089832	737.214280	10.690010
9.544997	743.014167	10.695015
9.528051	748.859397	10.700019
9.516175	745.797283	10.705024
9.521261	741.571840	10.710029
9.478324	754.897470	10.715034
9.332741	751.984414	10.720039
9.209200	756.160903	10.725043
9.627211	749.551499	10.730048
9.759311	763.905766	10.735053
9.408296	756.941206	10.740058
10.260417	769.835510	10.745063
10.152386	773.821874	10.750067
9.826756	760.293199	10.755072
10.118392	768.490894	10.760077
10.123803	758.865958	10.765082
10.292041	771.222797	10.770087
9.760893	768.495812	10.775091
10.314294	778.820052	10.780096
10.543425	778.663637	10.785101
10.325105	773.081381	10.790106
10.330554	765.851805	10.795111
10.351505	774.395449	10.800115
10.442206	782.770279	10.805120
10.454993	788.960863	10.810125
10.660735	772.713932	10.815130
10.788248	771.935065	10.820135
10.447027	773.438675	10.825139
10.557405	769.177507	10.830144
10.970042	780.531864	10.835149
10.659543	779.654126	10.840154
10.964679	779.668514	10.845159
10.830607	764.218531	10.850163
11.029924	755.253369	10.855168
10.784281	761.622354	10.860173
10.680100	764.682439	10.865178
11.279606	767.729635	10.870183
11.027521	789.993630	10.875187
11.032148	784.008382	10.880192
11.155486	780.968849	10.885197
10.921187	791.007153	10.890202
11.249544	777.924504	10.895207
11.088748	789.468099	10.900211
11.256344	783.169855	10.905216
10.917609	789.493777	10.910221
11.323094	795.735268	10.915226
11.628682	777.890734	10.920231
11.172726	783.919539	10.925235
11.258443	787.576963	10.930240
11.405537	782.896776	10.935245
11.038594	790.243900	10.940250
11.469204	789.091839	10.945255
11.436424	815.247476	10.950259
11.755217	808.068826	10.955264
11.823816	809.443996	10.960269
11.767355	810.134219	10.965274
12.175628	809.703229	10.970279
11.583076	819.024414	10.975283
11.753941	816.362068	10.980288
11.871073	821.499971	10.985293
11.971317	816.644320	10.990298
12.247249	819.195938	10.995303
12.031909	820.137006	11.000307
12.408683	817.129582	11.005312
12.105156	820.405977	11.010317
12.017844	828.577416	11.015322
12.451044	821.052506	11.020327
12.181358	820.904690	11.025331
12.416671	816.293999	11.030336
12.374800	818.189835	11.035341
12.312672	820.103095	11.040346
12.529069	815.935389	11.045351
12.483536	828.286950	11.050355
12.704191	818.894147	11.055360
12.716284	828.590405	11.060365
12.582381	827.605650	11.065370
12.827613	825.144328	11.070375
12.625544	830.514495	11.075379
12.836263	831.269337	11.080384
12.840126	839.938747	11.085389
12.865320	848.188446	11.090394
13.166048	849.982334	11.095399
13.191230	853.343502	11.100403
13.390688	839.261072	11.105408
13.066980	832.623278	11.110413
12.658037	832.437748	11.115418
13.438382	830.197003	11.120423
13.272680	849.171996	11.125427
13.074081	840.694446	11.130432
13.302167	854.397985	11.135437
13.298233	855.251720	11.140442
13.885692	854.484644	11.145447
13.458096	844.523439	11.150451
13.585932	846.940989	11.155456
13.309750	837.001370	11.160461
13.441341	849.677934	11.165466
13.697071	843.583226	11.170471
13.697319	851.595633	11.175475
13.663045	838.299533	11.180480
14.005852	851.182106	11.185485
14.002420	845.139771	11.190490
13.993219	852.745256	11.195495
14.109089	857.344058	11.200499
13.789746	831.820050	11.205504
13.535571	843.747587	11.210509
13.677450	854.334637	11.215514
14.129201	851.837218	11.220519
13.805857	865.502563	11.225523
13.816543	861.380271	11.230528
13.819566	850.465711	11.235533
13.960126	859.370372	11.240538
14.015822	850.852258	11.245543
13.874101	873.978715	11.250547
14.415167	871.120117	11.255552
14.663708	877.146981	11.260557
14.829815	876.792461	11.265562
14.838711	871.702203	11.270567
14.592357	865.640258	11.275571
14.682775	851.138393	11.280576
14.418829	850.874543	11.285581
14.373457	856.845774	11.290586
14.447227	868.793566	11.295591
14.412592	879.355171	11.300595
14.677777	883.476004	11.305600
14.907627	883.469285	11.310605
14.645643	891.274380	11.315610
14.989497	880.489940	11.320615
14.556210	880.372947	11.325619
15.019688	874.834870	11.330624
15.088845	880.276912	11.335629
15.375191	880.557649	11.340634
15.341587	879.739819	11.345639
15.235864	883.904041	11.350643
15.226968	872.644436	11.355648
15.581660	879.796082	11.360653
15.496122	888.957597	11.365658
15.509668	880.502958	11.370663
15.265770	880.535530	11.375667
15.141325	878.711902	11.380672
15.381766	887.198528	11.385677
15.179345	885.732688	11.390682
15.392018	876.172388	11.395687
15.191035	908.109313	11.400691
16.085459	904.819035	11.405696
15.930630	907.314795	11.410701
15.892019	896.906735	11.415706
16.026659	881.656618	11.420711
15.846812	886.476059	11.425715
15.581778	876.815332	11.430720
16.111390	897.456711	11.435725
15.987521	898.439964	11.440730
16.339083	902.975957	11.445735
15.814137	890.813051	11.450739
16.149134	903.269562	11.455744
16.332422	898.971496	11.460749
16.148571	909.856544	11.465754
16.318915	900.630985	11.470759
16.432309	902.850575	11.475763
16.657502	896.407477	11.480768
16.141624	891.363066	11.485773
16.127507	900.281384	11.490778
16.403592	903.843820	11.495783
16.049452	902.813763	11.500787
16.600894	905.105411	11.505792
16.886256	900.746909	11.510797
16.475213	907.405689	11.515802
16.948548	899.213595	11.520807
16.879288	918.066063	11.525811
17.111456	903.509998	11.530816
16.875137	915.366937	11.535821
16.768536	906.135084	11.540826
17.117889	904.205922	11.545831
16.769457	914.155282	11.550835
16.711621	899.747977	11.555840
17.025430	917.317207	11.560845
17.172253	902.014663	11.565850
17.302420	900.905784	11.570855
16.940521	907.947810	11.575859
17.147532	905.743307	11.580864
17.438096	900.866734	11.585869
17.054355	909.099690	11.590874
17.691415	888.420406	11.595879
17.212353	912.247279	11.600883
17.355437	901.382882	11.605888
17.409615	893.940466	11.610893
17.342175	908.807674	11.615898
17.267374	907.833987	11.620903
17.417343	912.304365	11.625907
17.677021	905.147712	11.630912
17.433175	905.093543	11.635917
17.922256	929.489851	11.640922
18.236938	919.974753	11.645927
17.843264	903.992014	11.650931
17.671153	905.675245	11.655936
18.080416	917.269946	11.660941
17.830436	917.920077	11.665946
18.219525	908.547660	11.670951
17.723173	919.305939	11.675955
18.163075	918.833632	11.680960
18.100946	937.923109	11.685965
17.979668	937.431497	11.690970
18.114911	934.766926	11.695975
18.245782	933.820358	11.700979
18.326050	937.153837	11.705984
18.322186	941.580950	11.710989
18.204180	937.359313	11.715994
18.394008	925.609077	11.720999
18.175296	942.686108	11.726003
18.821373	926.756705	11.731008
18.390068	938.340410	11.736013
18.548193	939.043723	11.741018
18.658596	926.166014	11.746023
18.696703	936.938411	11.751027
18.503990	937.934224	11.756032
18.799557	929.163339	11.761037
18.776538	950.343946	11.766042
18.487953	939.546792	11.771047
18.677740	949.946498	11.776051
19.045652	968.983196	11.781056
19.380451	964.575790	11.786061
19.117131	978.072394	11.791066
19.439274	954.803411	11.796071
19.235711	946.470094	11.801075
19.129722	943.670531	11.806080
19.255230	923.858112	11.811085
18.943007	931.696473	11.816090
19.441708	942.753381	11.821095
19.485544	957.115611	11.826099
19.869103	954.903442	11.831104
19.772496	945.248922	11.836109
19.430459	938.137760	11.841114
19.552404	938.446296	11.846119
19.370644	942.477583	11.851123
19.434622	927.547771	11.856128
19.889290	942.748057	11.861133
19.367858	948.552405	11.866138
19.998638	961.944237	11.871143
19.626052	970.441954	11.876147
19.580701	965.336661	11.881152
19.902570	955.981243	11.886157
20.042295	967.388739	11.891162
20.253079	948.431590	11.896167
20.330871	961.653000	11.901171
20.122338	958.393548	11.906176
20.068513	956.311064	11.911181
19.972352	952.117477	11.916186
20.620718	954.819454	11.921191
20.224631	960.886090	11.926195
20.060623	953.968877	11.931200
20.226914	955.799991	11.936205
20.086484	964.691187	11.941210
20.457120	945.252805	11.946215
20.187807	961.691377	11.951219
20.130406	952.757576	11.956224
20.374219	958.603879	11.961229
20.256407	961.446982	11.966234
20.737804	947.194899	11.971239
20.279156	962.160828	11.976243
20.618987	969.764323	11.981248
21.075635	974.608433	11.986253
20.646560	984.028228	11.991258
21.358648	968.715882	11.996263
21.220505	964.325560	12.001267
20.960500	956.843335	12.006272
21.024323	951.966640	12.011277
20.420530	953.718727	12.016282
20.938910	949.690477	12.021287
20.906079	958.742704	12.026291
21.186176	967.284554	12.031296
21.268734	963.469315	12.036301
21.003166	957.054003	12.041306
21.239463	952.204992	12.046311
20.902774	945.572369	12.051315
21.068966	942.647393	12.056320
20.962920	954.655475	12.061325
21.226222	945.698914	12.066330
21.605347	941.623491	12.071335
21.426393	942.624994	12.076339
21.127706	939.763126	12.081344
21.380329	942.078787	12.086349
21.070334	937.946118	12.091354
21.023894	920.993342	12.096359
20.742464	914.071222	12.101363
20.851091	929.653116	12.106368
21.119044	949.232435	12.111373
20.953524	947.058957	12.116378
21.323979	938.940021	12.121383
20.767169	929.626993	12.126387
20.956309	916.471806	12.131392
21.516365	919.239901	12.136397
20.924203	927.906656	12.141402
21.050972	922.136836	12.146407
21.052340	917.408886	12.151411
21.076684	917.133746	12.156416
20.888660	920.836442	12.161421
20.911521	924.035570	12.166426
21.276069	908.915913	12.171431
20.922568	914.259800	12.176435
21.099856	920.288585	12.181440
21.045244	913.262480	12.186445
20.818259	907.285737	12.191450
21.040169	914.417578	12.196455
20.852062	924.379221	12.201459
21.050773	912.674887	12.206464
21.001467	919.695447	12.211469
20.768064	928.349137	12.216474
21.272636	915.796500	12.221479
21.243212	918.459918	12.226483
21.177976	914.034328	12.231488
21.333465	918.737217	12.236493
21.124649	917.132045	12.241498
21.376787	922.636383	12.246503
20.839452	930.441262	12.251507
21.468934	911.455228	12.256512
21.271182	901.674943	12.261517
20.915772	892.733517	12.266522
20.676106	896.152707	12.271527
20.687370	903.425372	12.276531
20.769204	903.161563	12.281536
20.929179	917.017952	12.286541
20.912059	929.259412	12.291546
20.920355	917.716332	12.296551
20.855986	932.836965	12.301555
20.727110	926.675831	12.306560
21.020261	926.480821	12.311565
20.700603	934.536412	12.316570
21.142968	919.303407	12.321575
20.922673	925.274181	12.326579
20.969549	932.577452	12.331584
21.148587	933.501357	12.336589
20.891120	931.990675	12.341594
20.898043	932.344365	12.346599
20.914023	934.924850	12.351603
21.337616	929.730583	12.356608
21.478827	930.300975	12.361613
20.991682	935.678801	12.366618
20.926803	924.577896	12.371623
20.889139	925.001775	12.376627
21.146717	936.988116	12.381632
20.905275	922.239488	12.386637
20.817061	915.819560	12.391642
21.115834	927.964904	12.396647
21.100360	929.124837	12.401651
21.131685	915.818202	12.406656
21.238477	901.051900	12.411661
21.032284	907.742662	12.416666
20.889133	912.166751	12.421671
20.926226	904.845326	12.426675
20.903483	896.159922	12.431680
21.107480	909.574044	12.436685
20.605119	907.334447	12.441690
21.151915	892.154200	12.446695
20.942931	910.436011	12.451699
20.586164	901.097403	12.456704
21.054733	921.007386	12.461709
20.964070	923.205908	12.466714
21.298874	923.704422	12.471719
20.847624	920.097337	12.476723
20.863677	906.616527	12.481728
21.259193	909.606406	12.486733
21.019727	907.815312	12.491738
21.251592	909.680116	12.496743
20.572808	903.581468	12.501747
20.682597	910.040484	12.506752
20.923393	903.281082	12.511757
20.797694	936.478664	12.516762
21.275450	922.839045	12.521767
20.943147	934.101027	12.526771
21.112130	929.399956	12.531776
21.187365	913.367648	12.536781
20.675806	916.475393	12.541786
21.036940	901.619639	12.546791
20.706235	921.504138	12.551795
21.366145	922.671468	12.556800
21.290887	910.118276	12.561805
20.831823	918.349058	12.566810
21.233166	908.829607	12.571815
21.228275	908.677401	12.576819
21.215645	905.528641	12.581824
21.400518	908.654618	12.586829
21.377237	911.826411	12.591834
21.468383	906.043355	12.596839
21.285223	909.737388	12.601843
20.758016	897.287829	12.606848
20.890453	884.157485	12.611853
20.846824	905.890094	12.616858
20.974300	908.862799	12.621863
21.066149	908.149538	12.626867
20.766008	908.719359	12.631872
21.017627	917.462841	12.636877
20.836970	916.138607	12.641882
21.222540	907.203569	12.646887
21.075203	913.061777	12.651891
20.845564	911.105112	12.656896
21.268050	908.814202	12.661901
20.798260	898.941689	12.666906
20.685843	913.242065	12.671911
21.011769	907.560335	12.676915
20.775937	912.532217	12.681920
20.677218	918.347979	12.686925
20.526316	912.431639	12.691930
21.035679	918.385382	12.696935
20.708637	919.222846	12.701939
20.681268	915.092415	12.706944
21.106003	910.620218	12.711949
20.708718	912.364595	12.716954
20.934367	905.241753	12.721959
20.843817	909.723684	12.726963
20.858049	921.088081	12.731968
21.123028	913.271411	12.736973
20.844125	933.196549	12.741978
21.053614	913.749218	12.746983
20.784968	921.814013	12.751987
20.941050	924.391074	12.756992
21.096468	924.292148	12.761997
20.950401	929.454723	12.767002
21.061453	921.730407	12.772007
21.009468	926.676125	12.777011
21.205505	927.609934	12.782016
21.036485	922.150643	12.787021
20.837573	928.852869	12.792026
20.902714	925.660162	12.797031
21.145133	927.485438	12.802035
21.309061	926.763834	12.807040
21.122403	921.032965	12.812045
20.972313	918.792375	12.817050
21.071366	916.978828	12.822055
20.871395	913.016275	12.827059
20.810282	925.655833	12.832064
21.071778	921.889336	12.837069
20.805005	928.343765	12.842074
21.010522	918.595343	12.847079
20.925954	921.374789	12.852083
20.944629	918.646812	12.857088
21.031683	926.424642	12.862093
21.246227	918.950327	12.867098
20.984845	927.051814	12.872103
21.237378	924.595619	12.877107
20.918254	930.613697	12.882112
21.366640	917.302043	12.887117
20.868280	929.858379	12.892122
21.085402	909.889441	12.897127
21.044444	922.666130	12.902131
21.054015	920.234495	12.907136
21.275376	922.064706	12.912141
20.860937	933.847567	12.917146
20.880164	918.013422	12.922151
21.018276	930.638555	12.927155
21.019518	912.605854	12.932160
21.317606	925.790518	12.937165
20.657570	917.052205	12.942170
20.749399	896.735838	12.947175
20.993986	925.950881	12.952179
21.092754	929.476949	12.957184
21.516342	925.517441	12.962189
20.907707	902.701348	12.967194
20.788934	900.864197	12.972199
20.692323	896.123495	12.977203
20.793753	909.114006	12.982208
21.308269	918.304413	12.987213
20.926357	936.019325	12.992218
21.191485	916.933701	12.997223
21.081236	913.224920	13.002227
20.920420	903.924444	13.007232
21.112455	897.425134	13.012237
21.150599	906.917017	13.017242
20.851552	894.784308	13.022247
20.926816	899.567796	13.027251
20.818420	897.959225	13.032256
21.070408	890.193525	13.037261
20.717529	905.637689	13.042266
21.150572	895.939725	13.047271
20.960263	900.650453	13.052275
20.804075	888.018725	13.057280
20.927525	909.361992	13.062285
20.955321	924.715499	13.067290
21.037803	924.697592	13.072295
20.994897	935.517601	13.077299
21.028491	917.545966	13.082304
20.937742	908.831977	13.087309
20.603932	921.152326	13.092314
21.286371	923.766861	13.097319
21.244050	931.248361	13.102323
20.831261	927.034318	13.107328
21.043879	908.982101	13.112333
20.885649	915.393981	13.117338
21.122101	899.266590	13.122343
20.710903	912.275786	13.127347
20.696550	911.735582	13.132352
21.155143	930.811384	13.137357
21.109445	936.046262	13.142362
21.034879	922.444273	13.147367
21.087490	925.966664	13.152371
20.561435	910.547503	13.157376
20.882577	912.112639	13.162381
21.059090	940.174776	13.167386
21.153233	932.304918	13.172391
20.766084	932.188449	13.177395
21.184379	941.154521	13.182400
21.297263	934.336657	13.187405
21.198461	924.326109	13.192410
20.855879	914.352871	13.197415
21.031043	912.557147	13.202419
20.867601	912.143224	13.207424
20.864708	913.872006	13.212429
20.779366	915.371087	13.217434
20.840405	906.123535	13.222439
20.592593	925.567464	13.227443
20.882269	931.863757	13.232448
21.299026	938.253326	13.237453
21.042306	946.652125	13.242458
21.443997	932.925280	13.247463
20.876953	919.485420	13.252467
21.148387	917.839920	13.257472
21.401009	910.340613	13.262477
20.784663	915.160297	13.267482
20.782007	912.848884	13.272487
21.004386	918.042576	13.277491
20.795763	917.372507	13.282496
20.872226	910.522617	13.287501
20.530142	925.562958	13.292506
21.085834	930.033286	13.297511
21.426576	943.622749	13.302515
21.114884	924.883004	13.307520
20.719758	922.127984	13.312525
20.774791	921.980413	13.317530
20.977823	914.771289	13.322535
20.760514	924.806975	13.327539
20.986998	938.506120	13.332544
21.342387	950.760725	13.337549
21.214021	936.465557	13.342554
20.749445	930.961938	13.347559
21.015105	920.886954	13.352563
21.166481	922.004505	13.357568
21.168174	920.466683	13.362573
20.945724	932.157420	13.367578
21.074046	916.671731	13.372583
21.045052	930.954088	13.377587
20.906448	914.992155	13.382592
21.191102	921.536827	13.387597
20.717714	925.704508	13.392602
20.883473	918.526557	13.397607
20.936012	918.477156	13.402611
20.874896	918.852736	13.407616
20.723485	914.932900	13.412621
20.731260	910.314317	13.417626
20.893584	929.200827	13.422631
21.073401	939.986894	13.427635
20.878150	931.325829	13.432640
21.253002	921.452626	13.437645
21.093732	931.895377	13.442650
20.963824	915.026884	13.447655
20.774423	922.042981	13.452659
20.844265	923.996707	13.457664
21.117180	915.199481	13.462669
20.835943	926.390234	13.467674
21.041400	920.413899	13.472679
21.268521	917.196935	13.477683
20.867599	923.224903	13.482688
21.051946	909.969561	13.487693
20.921872	916.667111	13.492698
21.109655	915.383460	13.497703
20.840297	924.527007	13.502707
20.874701	932.322700	13.507712
20.960637	920.935968	13.512717
20.764800	931.567478	13.517722
21.160405	930.741113	13.522727
21.074032	931.347804	13.527731
21.291159	927.321876	13.532736
21.018525	921.797109	13.537741
21.273270	913.535793	13.542746
21.051332	923.222133	13.547751
21.200879	932.019751	13.552755
21.097153	927.016822	13.557760
21.101646	926.144028	13.562765
20.636843	940.617330	13.567770
20.904746	927.143641	13.572775
20.969491	927.003983	13.577779
21.134396	937.071758	13.582784
21.144822	930.891559	13.587789
20.788590	929.330398	13.592794
20.953294	932.339748	13.597799
21.133969	927.102224	13.602803
20.838454	932.933611	13.607808
21.548982	926.119779	13.612813
21.375125	935.350603	13.617818
20.960023	929.733438	13.622823
21.061791	931.167985	13.627827
21.187374	930.875120	13.632832
21.089277	933.294027	13.637837
21.117620	928.186455	13.642842
20.975413	910.321716	13.647847
20.533058	916.551831	13.652851
20.598511	915.339732	13.657856
20.971280	924.573251	13.662861
20.765532	939.178699	13.667866
21.172535	938.260629	13.672871
21.032131	934.842082	13.677875
20.722128	946.672952	13.682880
20.974217	938.754245	13.687885
20.838484	933.166638	13.692890
21.117947	926.716448	13.697895
21.145766	935.900914	13.702899
21.236814	944.990145	13.707904
21.234401	934.948446	13.712909
21.037439	947.284837	13.717914
20.840653	929.906597	13.722919
20.922347	928.627250	13.727923
20.858774	937.632328	13.732928
21.194996	949.479980	13.737933
21.075335	955.124055	13.742938
21.171102	934.975741	13.747943
21.126817	915.983622	13.752947
21.045669	918.489709	13.757952
21.218108	914.688533	13.762957
21.110885	907.621936	13.767962
21.241471	909.564394	13.772967
21.187157	913.130644	13.777971
20.824895	907.208593	13.782976
20.938565	911.468718	13.787981
20.827284	913.005052	13.792986
21.066566	901.177562	13.797991
21.102593	907.741382	13.802995
20.854416	917.920760	13.808000
20.732486	907.369862	13.813005
20.610126	913.422782	13.818010
20.955457	905.333103	13.823015
20.825719	910.294370	13.828019
20.673156	909.347279	13.833024
20.885306	915.315308	13.838029
20.505839	925.648095	13.843034
21.349956	922.561381	13.848039
21.114426	944.252115	13.853043
20.895446	931.053198	13.858048
21.307282	930.175359	13.863053
20.976530	923.136521	13.868058
20.918765	914.753159	13.873063
20.962775	911.675789	13.878067
20.819944	914.388833	13.883072
20.819286	913.958408	13.888077
21.182329	939.155429	13.893082
21.171280	933.611013	13.898087
21.136120	930.240336	13.903091
20.919749	927.813197	13.908096
21.091285	911.882226	13.913101
20.802943	915.433764	13.918106
20.872552	921.421376	13.923111
20.916349	924.801670	13.928115
21.002049	913.771373	13.933120
21.217776	913.095124	13.938125
21.150795	913.766530	13.943130
21.264184	912.318127	13.948135
21.043152	907.136796	13.953139
20.925865	910.410314	13.958144
21.131396	915.365418	13.963149
21.148003	913.315861	13.968154
20.882897	914.789998	13.973159
20.864177	918.413650	13.978163
20.727087	918.561651	13.983168
21.247133	914.466913	13.988173
21.058014	924.734646	13.993178
20.918710	918.422215	13.998183
20.946674	921.251522	14.003187
20.755589	918.549115	14.008192
20.945550	918.450214	14.013210
21.075683	918.121143	14.018227
21.108241	919.992437	14.023245
20.782779	919.698280	14.028263
20.795107	925.295932	14.033280
21.031941	913.833932	14.038298
20.841517	915.769102	14.043315
20.915606	918.355748	14.048333
21.177220	926.872326	14.053351
20.856079	917.581880	14.058368
21.083236	930.572656	14.063386
21.415728	944.293787	14.068403
21.180023	930.388873	14.073421
21.385144	933.934559	14.078439
20.748113	933.298435	14.083456
20.700191	933.499528	14.088474
21.182971	947.149504	14.093491
21.229603	943.607661	14.098509
21.039014	945.792958	14.103527
21.222184	948.327607	14.108544
21.501720	941.928344	14.113562
21.381758	946.026076	14.118579
21.465133	935.768236	14.123597
21.725401	949.996366	14.128615
21.317791	957.897723	14.133632
21.418814	942.929265	14.138650
21.225867	954.805793	14.143667
21.010864	941.355291	14.148685
21.462930	944.021647	14.153703
21.414902	946.829110	14.158720
21.545124	954.934104	14.163738
21.356975	952.197297	14.168755
21.563826	950.673142	14.173773
21.513081	952.702436	14.178791
21.638891	951.581294	14.183808
21.378994	941.285396	14.188826
21.155287	963.052734	14.193843
21.409858	967.553179	14.198861
21.519964	976.764023	14.203879
21.605151	982.117281	14.208896
21.814482	973.165312	14.213914
21.959417	984.679679	14.218931
21.960864	983.510733	14.223949
22.042806	983.991546	14.228967
21.821157	973.264831	14.233984
21.943187	960.737350	14.239002
22.062367	950.078982	14.244019
21.500602	960.235349	14.249037
21.963044	943.510475	14.254055
21.708478	947.167233	14.259072
21.681135	954.127093	14.264090
21.639029	958.976858	14.269107
21.864620	981.687107	14.274125
22.019541	978.069785	14.279143
21.715634	975.708494	14.284160
22.364010	979.567292	14.289178
22.026409	985.420542	14.294195
22.010171	978.001986	14.299213
22.303461	971.572204	14.304231
21.537243	980.638117	14.309248
21.737914	984.807409	14.314266
21.826009	985.755976	14.319283
21.873666	984.332709	14.324301
22.195522	992.142906	14.329319
21.854719	989.384824	14.334336
22.217347	981.926287	14.339354
22.164058	987.809693	14.344371
21.946105	980.050521	14.349389
22.617174	978.900610	14.354407
22.187666	988.155057	14.359424
22.235196	984.476214	14.364442
22.104665	992.349126	14.369459
22.284475	980.395974	14.374477
22.536243	976.907916	14.379495
22.314249	992.403720	14.384512
22.399444	981.837261	14.389530
22.363666	999.129554	14.394547
22.221809	989.892259	14.399565
22.375802	982.787877	14.404583
22.114789	986.418933	14.409600
21.960534	983.728622	14.414618
22.150856	986.446170	14.419635
22.293908	1004.483834	14.424653
22.680523	1004.744603	14.429671
22.511827	1016.590574	14.434688
22.719896	1007.105558	14.439706
22.789670	1007.663813	14.444723
22.546539	1008.677793	14.449741
22.576349	989.012832	14.454759
22.453900	1002.996906	14.459776
22.782262	999.727849	14.464794
22.757436	997.977958	14.469811
22.758962	977.106360	14.474829
22.636827	979.600051	14.479847
22.363790	986.762699	14.484864
22.438055	1003.770047	14.489882
22.868731	996.017520	14.494899
22.995240	1002.407055	14.499917
22.921978	998.163914	14.504935
23.098378	1004.841205	14.509952
22.807384	995.149519	14.514970
22.904813	988.076178	14.519987
22.712437	990.518156	14.525005
22.989640	981.538054	14.530023
22.999993	1012.159960	14.535040
22.792421	991.117209	14.540058
22.831641	992.685446	14.545075
22.649173	1002.144305	14.550093
23.098151	1005.827286	14.555111
23.035549	1008.687420	14.560128
23.077474	1006.157713	14.565146
23.062822	1013.471063	14.570163
23.155643	1006.036671	14.575181
23.546056	1007.888651	14.580199
23.278582	990.707589	14.585216
23.083375	988.870050	14.590234
23.250151	980.756949	14.595251
22.656377	980.656587	14.600269
22.890093	991.058887	14.605287
22.943011	1000.022478	14.610304
23.477795	1008.325658	14.615322
23.296500	1007.439100	14.620339
23.322140	1007.554533	14.625357
23.649670	1012.892745	14.630375
23.325138	1006.283076	14.635392
22.989646	999.145077	14.640410
23.152932	1011.005730	14.645427
22.964326	1018.749500	14.650445
22.933824	1002.345414	14.655463
22.895843	1002.168989	14.660480
23.215669	1010.611842	14.665498
23.175596	996.469606	14.670515
23.404457	1008.110598	14.675533
23.445641	999.361601	14.680551
23.368806	1009.097757	14.685568
23.914974	1017.290594	14.690586
23.715555	1005.921694	14.695603
23.488742	1020.150506	14.700621
23.773975	997.783375	14.705639
23.610837	1012.220662	14.710656
23.579659	1006.632233	14.715674
23.671251	1008.404465	14.720691
23.760586	1013.595061	14.725709
23.832074	1009.110190	14.730727
23.478912	1006.714280	14.735744
23.426632	1007.395816	14.740762
23.711317	995.650855	14.745779
23.438327	1013.753313	14.750797
24.132550	1016.698796	14.755815
24.012354	1015.027032	14.760832
24.059394	1010.868513	14.765850
23.945390	1009.607873	14.770867
23.771675	1009.473546	14.775885
24.001764	1005.792321	14.780903
23.852974	999.714592	14.785920
23.856722	1006.074947	14.790938
23.756136	1001.617524	14.795955
23.780547	1017.058325	14.800973
23.870478	1018.898460	14.805991
23.927280	1035.441467	14.811008
24.122697	1040.234500	14.816026
24.206922	1037.257617	14.821043
24.376373	1032.436235	14.826061
24.524834	1014.134934	14.831079
24.280942	1008.953217	14.836096
24.380087	996.833600	14.841114
24.517068	1000.821158	14.846131
24.306225	1006.761159	14.851149
24.371325	1002.164058	14.856167
24.502954	997.126935	14.861184
24.432965	1005.057834	14.866202
24.307513	985.648863	14.871219
24.395427	1000.337091	14.876237
24.468101	998.950728	14.881255
24.190022	1013.747678	14.886272
24.025984	1008.741978	14.891290
24.537447	999.759107	14.896307
24.240421	1001.649946	14.901325
24.208344	1003.542571	14.906343
24.046755	999.722481	14.911360
24.301868	994.843406	14.916378
24.319283	1003.749744	14.921395
24.061959	1003.009012	14.926413
24.164333	1000.683586	14.931431
24.355166	1005.079385	14.936448
24.280986	1008.345611	14.941466
24.904944	1013.726203	14.946483
24.747403	1022.130374	14.951501
24.741732	1002.371958	14.956519
24.631976	1015.481037	14.961536
24.809521	1004.516034	14.966554
24.714285	1007.862692	14.971571
24.478326	1011.467737	14.976589
24.680640	1008.259678	14.981607
24.519638	997.428896	14.986624
24.693714	1012.526515	14.991642
24.961040	1019.742988	14.996659
24.723105	1018.997590	15.001677
24.861284	1030.961360	15.006695
24.985345	1033.719372	15.011712
25.056564	1017.404431	15.016730
24.796939	1015.253137	15.021747
24.746625	1017.851777	15.026765
24.866920	1034.881706	15.031783
24.983755	1032.678231	15.036800
25.015739	1043.987301	15.041818
24.998633	1037.883835	15.046835
24.921680	1045.350275	15.051853
24.775857	1042.119088	15.056871
24.889961	1044.052893	15.061888
25.023778	1049.162479	15.066906
24.676144	1038.385026	15.071923
24.849097	1041.721950	15.076941
25.148596	1046.701296	15.081959
24.954332	1044.654397	15.086976
24.802098	1046.240591	15.091994
25.301490	1028.625731	15.097011
25.284455	1033.429052	15.102029
25.058092	1044.522938	15.107047
25.205945	1044.279123	15.112064
24.971470	1055.424645	15.117082
25.016894	1052.490126	15.122099
25.259314	1071.742069	15.127117
25.329754	1061.503505	15.132135
25.335391	1066.224574	15.137152
25.230929	1070.087072	15.142170
25.373224	1059.904686	15.147187
25.531444	1070.879055	15.152205
26.003355	1064.309064	15.157223
25.900366	1065.939314	15.162240
25.939760	1059.902328	15.167258
26.000160	1029.382246	15.172275
25.550164	1024.378107	15.177293
25.805513	1022.817896	15.182311
25.949933	1035.118857	15.187328
25.644368	1032.808155	15.192346
25.940263	1031.010253	15.197363
25.949135	1034.502327	15.202381
25.841969	1026.549290	15.207399
25.879900	1037.416983	15.212416
25.683752	1028.432129	15.217434
25.927729	1022.071535	15.222451
25.714824	1032.356345	15.227469
25.714420	1027.871925	15.232487
26.023444	1017.197385	15.237504
25.900691	1034.085189	15.242522
26.129906	1025.614484	15.247539
25.969429	1026.225193	15.252557
25.962160	1032.142173	15.257575
25.645944	1027.610600	15.262592
25.374418	1028.802134	15.267610
25.887274	1022.612576	15.272627
25.442447	1028.135324	15.277645
25.734473	1022.408828	15.282663
25.851879	1023.011394	15.287680
25.540321	1029.780680	15.292698
25.855428	1044.159025	15.297715
25.718151	1048.783338	15.302733
25.891478	1056.452100	15.307751
25.908270	1051.615735	15.312768
26.059930	1057.842416	15.317786
26.464068	1046.256105	15.322803
26.650286	1051.528785	15.327821
26.429231	1059.472797	15.332839
26.631134	1053.219569	15.337856
26.208049	1058.841102	15.342874
26.197902	1043.416814	15.347891
26.275254	1059.423342	15.352909
26.196543	1047.522377	15.357927
26.238042	1054.208624	15.362944
26.148071	1059.368062	15.367962
26.220729	1051.889674	15.372979
26.550427	1050.281424	15.377997
26.555160	1058.820176	15.383015
26.965319	1047.906125	15.388032
26.777580	1065.342278	15.393050
26.633106	1051.496625	15.398067
26.238697	1051.611416	15.403085
26.508555	1054.995805	15.408103
26.952928	1059.557239	15.413120
26.646378	1048.943104	15.418138
26.618458	1050.655756	15.423155
26.558780	1052.754126	15.428173
26.495083	1046.255412	15.433191
26.600717	1058.575163	15.438208
26.756288	1055.206244	15.443226
26.769922	1051.484030	15.448243
26.592201	1062.309062	15.453261
26.827396	1042.331286	15.458279
26.543030	1056.854016	15.463296
26.577946	1079.634155	15.468314
26.935071	1075.638510	15.473331
27.350297	1085.197142	15.478349
27.193898	1078.403328	15.483367
27.340198	1059.707504	15.488384
27.048080	1056.600314	15.493402
26.866482	1051.268654	15.498419
26.911407	1051.539879	15.503437
27.050827	1046.940348	15.508455
27.021731	1056.554098	15.513472
27.387575	1077.291674	15.518490
27.340889	1059.704100	15.523507
27.403049	1055.892351	15.528525
26.905163	1051.229305	15.533543
27.272257	1044.369316	15.538560
26.557935	1060.434475	15.543578
26.846609	1074.477309	15.548595
27.271009	1079.927506	15.553613
27.531162	1082.110143	15.558631
27.745768	1077.418390	15.563648
27.481277	1077.735820	15.568666
27.786173	1079.442582	15.573683
27.542824	1068.533648	15.578701
27.671118	1044.074288	15.583719
27.632141	1045.404904	15.588736
27.442029	1050.525258	15.593754
27.716915	1045.072033	15.598771
27.668803	1038.212206	15.603789
27.412527	1037.098517	15.608807
27.764473	1043.400208	15.613824
27.245021	1049.380009	15.618842
27.771534	1046.986929	15.623859
27.404744	1040.744188	15.628877
27.236332	1053.375043	15.633895
27.411250	1061.082877	15.638912
27.295813	1076.676602	15.643930
27.487340	1078.802547	15.648947
27.465231	1085.174926	15.653965
27.773300	1072.281066	15.658983
27.661067	1073.228557	15.664000
27.404877	1080.550578	15.669018
27.720439	1075.888340	15.674035
27.576289	1081.131929	15.679053
27.558330	1094.679448	15.684071
28.188951	1097.333085	15.689088
28.262308	1099.811347	15.694106
28.435077	1083.851352	15.699123
27.590593	1087.830309	15.704141
28.144311	1087.059314	15.709159
28.604754	1090.534432	15.714176
27.973652	1091.877698	15.719194
27.799986	1083.093707	15.724211
28.305423	1078.368153	15.729229
28.105283	1082.768133	15.734247
28.433210	1067.941100	15.739264
27.921670	1082.734458	15.744282
28.255084	1088.966769	15.749299
28.422622	1084.604976	15.754317
28.166710	1089.056323	15.759335
28.250853	1088.655936	15.764352
28.327436	1092.366875	15.769370
28.380286	1097.766231	15.774387
28.713656	1093.052386	15.779405
28.446296	1087.921571	15.784423
28.489726	1076.995206	15.789440
28.516787	1068.839848	15.794458
28.354862	1078.982860	15.799475
28.419280	1080.319010	15.804493
28.149658	1085.960119	15.809511
28.524706	1091.533017	15.814528
28.556089	1100.083273	15.819546
28.891217	1090.258629	15.824563
29.107456	1078.200489	15.829581
28.749512	1092.818357	15.834599
29.005107	1085.999726	15.839616
28.975450	1073.208491	15.844634
28.819692	1066.663106	15.849651
28.670872	1065.518120	15.854669
28.693951	1065.844737	15.859687
28.938178	1061.561951	15.864704
28.671477	1067.671326	15.869722
28.617956	1061.663315	15.874739
28.823726	1077.707582	15.879757
28.743442	1081.649593	15.884775
29.247420	1095.052523	15.889792
28.906579	1087.427718	15.894810
29.065223	1090.422459	15.899827
28.893360	1088.696009	15.904845
28.837815	1090.650587	15.909863
29.140846	1080.500749	15.914880
29.203172	1098.469612	15.919898
29.132497	1097.644053	15.924915
29.260370	1083.618084	15.929933
29.015712	1097.942623	15.934951
29.050046	1089.782947	15.939968
28.903631	1086.216805	15.944986
29.003133	1093.143918	15.950003
28.978707	1084.666444	15.955021
28.976978	1090.757162	15.960039
29.132126	1075.794091	15.965056
29.172845	1091.007439	15.970074
28.917659	1091.908522	15.975091
29.137510	1103.753939	15.980109
29.196585	1118.080389	15.985127
29.360040	1112.563118	15.990144
29.585379	1120.989647	15.995162
29.547617	1130.269788	16.000179
29.622625	1114.336362	16.005197
29.568519	1121.453148	16.010215
29.697670	1112.834765	16.015232
29.659185	1119.538517	16.020250
29.626812	1121.877923	16.025267
29.992640	1121.843150	16.030285
29.860550	1122.274737	16.035303
29.912095	1107.620726	16.040320
29.950654	1115.090801	16.045338
29.521281	1105.745138	16.050355
29.847353	1114.540971	16.055373
29.609865	1122.895034	16.060391
29.842763	1106.406349	16.065408
30.105696	1123.967313	16.070426
29.836880	1108.798132	16.075443
30.188609	1112.992133	16.080461
30.060009	1120.374045	16.085479
30.163297	1109.328001	16.090496
30.384097	1113.618385	16.095514
30.074229	1101.898954	16.100531
29.843015	1088.507525	16.105549
29.721479	1101.099486	16.110567
30.307619	1105.070489	16.115584
29.847994	1108.513038	16.120602
29.619026	1112.525960	16.125619
29.976035	1106.271566	16.130637
29.762928	1111.955579	16.135655
29.728799	1107.163496	16.140672
30.002942	1119.978644	16.145690
30.148168	1132.290570	16.150707
30.542919	1133.721897	16.155725
30.084758	1137.392298	16.160743
30.747277	1124.781618	16.165760
30.837777	1136.782967	16.170778
30.620397	1126.909571	16.175795
30.558432	1111.661781	16.180813
30.411156	1104.503147	16.185831
30.096134	1100.592676	16.190848
30.693446	1117.014965	16.195866
30.225049	1123.954020	16.200883
30.506572	1132.933141	16.205901
30.459045	1134.976104	16.210919
30.612488	1133.614598	16.215936
30.668705	1131.466392	16.220954
30.578026	1130.351451	16.225971
30.759585	1126.780179	16.230989
30.987810	1130.838160	16.236007
30.956165	1119.834077	16.241024
30.964599	1130.110395	16.246042
30.861621	1131.717056	16.251059
31.007357	1127.346144	16.256077
31.145923	1138.734240	16.261095
31.024464	1123.057072	16.266112
31.153616	1132.796637	16.271130
30.745655	1126.497506	16.276147
31.190454	1120.642790	16.281165
30.883315	1128.042171	16.286183
31.081139	1131.651990	16.291200
31.118411	1121.487883	16.296218
30.941648	1127.181835	16.301235
31.616003	1123.572865	16.306253
31.157791	1128.537813	16.311271
31.352285	1117.609344	16.316288
31.430196	1122.982692	16.321306
31.241929	1127.747290	16.326323
31.448483	1118.130316	16.331341
31.153565	1132.714577	16.336359
31.100383	1124.966797	16.341376
31.219260	1136.812617	16.346394
31.255510	1136.765917	16.351411
31.387081	1120.810879	16.356429
31.114656	1128.240901	16.361447
31.093942	1120.258294	16.366464
31.383774	1122.771244	16.371482
31.237156	1130.524106	16.376499
31.175822	1122.889307	16.381517
31.497538	1145.634819	16.386535
31.923213	1145.505562	16.391552
32.205955	1144.074671	16.396570
31.800283	1140.420882	16.401587
31.542458	1126.953440	16.406605
31.711934	1119.660914	16.411623
31.625376	1119.644812	16.416640
32.095151	1124.911618	16.421658
31.670315	1128.263684	16.426675
31.693922	1117.997944	16.431693
31.635531	1138.951129	16.436711
31.867818	1142.975434	16.441728
32.147055	1152.975780	16.446746
31.948804	1149.609790	16.451763
32.500338	1141.159967	16.456781
31.914341	1143.899119	16.461799
32.126308	1153.008891	16.466816
31.909010	1139.335208	16.471834
32.078663	1145.238175	16.476851
32.137625	1143.827245	16.481869
32.622778	1140.485963	16.486887
32.143923	1147.348049	16.491904
32.445951	1133.832206	16.496922
31.972275	1141.417023	16.501939
32.314059	1137.431674	16.506957
32.238517	1145.203094	16.511975
32.301439	1150.031453	16.516992
32.584501	1140.773479	16.522010
32.378717	1146.372971	16.527027
32.869541	1133.215539	16.532045
32.379409	1136.354660	16.537063
32.184689	1131.309768	16.542080
32.515710	1136.288837	16.547098
32.477365	1150.124364	16.552115
32.564403	1140.444643	16.557133
32.587125	1143.759936	16.562151
32.280246	1143.415619	16.567168
32.918221	1141.083396	16.572186
32.332148	1143.934240	16.577203
32.356642	1149.460828	16.582221
32.494223	1139.088810	16.587239
32.781424	1151.711577	16.592256
32.657867	1147.776847	16.597274
32.346249	1152.164742	16.602291
32.832244	1141.428854	16.607309
32.713869	1151.675078	16.612327
32.777057	1160.997338	16.617344
33.397182	1169.801361	16.622362
32.809219	1166.944242	16.627379
33.048248	1168.101547	16.632397
33.168973	1177.150384	16.637415
33.091374	1170.900786	16.642432
33.549272	1159.900390	16.647450
33.014523	1166.990040	16.652467
33.103414	1156.952951	16.657485
33.042285	1157.572987	16.662503
32.882002	1168.892372	16.667520
33.312235	1165.536249	16.672538
33.223318	1175.211526	16.677555
33.110095	1189.891129	16.682573
33.306275	1178.860104	16.687591
32.913975	1190.436724	16.692608
33.189832	1176.185725	16.697626
33.173239	1185.213998	16.702643
33.372973	1168.799742	16.707661
33.321276	1177.160382	16.712679
32.744709	1187.637003	16.717696
33.763004	1194.131348	16.722714
33.358107	1201.536919	16.727731
33.762347	1195.949755	16.732749
33.942673	1211.391065	16.737767
33.980947	1214.398739	16.742784
33.979469	1195.628784	16.747802
33.844288	1208.081448	16.752819
33.967845	1176.121159	16.757837
33.542924	1177.143695	16.762855
33.568327	1183.741338	16.767872
34.017824	1202.608088	16.772890
34.105594	1202.837877	16.777907
34.235923	1197.336869	16.782925
34.104498	1174.721325	16.787943
33.789134	1171.315809	16.792960
33.810682	1158.050735	16.797978
33.884328	1173.560927	16.802995
34.064844	1189.936522	16.808013
34.135970	1194.577978	16.813031
33.921601	1207.059000	16.818048
34.299180	1202.702997	16.823066
33.993704	1200.227091	16.828083
33.989294	1201.811746	16.833101
33.832455	1194.446962	16.838119
33.760164	1205.859304	16.843136
33.893170	1190.180802	16.848154
33.664086	1215.167655	16.853171
34.105267	1211.139692	16.858189
34.126679	1229.903300	16.863207
34.111219	1234.767782	16.868224
34.420660	1224.715919	16.873242
34.442989	1232.298750	16.878259
34.521796	1233.870137	16.883277
34.932276	1221.282270	16.888295
34.801016	1222.896597	16.893312
34.952435	1218.488573	16.898330
34.913284	1220.080345	16.903347
34.869440	1223.886027	16.908365
35.240625	1213.308391	16.913383
34.958348	1229.536054	16.918400
34.961254	1205.348094	16.923418
34.842099	1209.428468	16.928435
34.898029	1210.165111	16.933453
34.884023	1203.033935	16.938471
34.599517	1215.294925	16.943488
34.995209	1221.441860	16.948506
34.807383	1221.857171	16.953523
35.254342	1215.199862	16.958541
35.433455	1217.793406	16.963559
34.871279	1217.467783	16.968576
35.148531	1213.349566	16.973594
35.085534	1211.901455	16.978611
35.387717	1217.747136	16.983629
35.330300	1212.741662	16.988647
35.197997	1223.278010	16.993664
35.287143	1217.752102	16.998682
35.292176	1222.166590	17.003699
35.246788	1225.862412	17.008717
35.290744	1206.798916	17.013735
35.532027	1226.579765	17.018752
35.454673	1217.509781	17.023770
35.138379	1214.283721	17.028787
35.355880	1215.018190	17.033805
35.451726	1216.476750	17.038823
35.333632	1218.949388	17.043840
35.425997	1214.667184	17.048858
35.299014	1211.023982	17.053875
35.063944	1216.923889	17.058893
35.660681	1206.101081	17.063911
35.523058	1229.594787	17.068928
35.960525	1234.874652	17.073946
35.995150	1242.189697	17.078963
35.724736	1229.422564	17.083981
35.960879	1219.048926	17.088999
35.610014	1214.345074	17.094016
35.966127	1220.487310	17.099034
35.987178	1238.576184	17.104051
36.151656	1238.866097	17.109069
35.915150	1235.923024	17.114087
36.081742	1241.577990	17.119104
36.214450	1248.386628	17.124122
36.188952	1232.963013	17.129139
35.909304	1217.049859	17.134157
36.275189	1229.196120	17.139175
36.040371	1245.729251	17.144192
36.078059	1236.161153	17.149210
36.156598	1243.036628	17.154227
35.875130	1242.121987	17.159245
36.266143	1243.122930	17.164263
36.445053	1235.010898	17.169280
36.342263	1243.670724	17.174298
36.442020	1245.325284	17.179315
36.479426	1243.529260	17.184333
36.352372	1239.991451	17.189351
36.185978	1251.996116	17.194368
36.194265	1236.792043	17.199386
36.147799	1238.449475	17.204403
36.477560	1249.025401	17.209421
36.856906	1257.915069	17.214439
37.052639	1259.810718	17.219456
37.098469	1255.043584	17.224474
37.254615	1241.030256	17.229491
36.782978	1235.707034	17.234509
37.237022	1229.341160	17.239527
36.450396	1228.801232	17.244544
36.648901	1226.496616	17.249562
36.766960	1223.676315	17.254579
36.669976	1244.347956	17.259597
36.875496	1246.102048	17.264615
37.016865	1265.494632	17.269632
36.877319	1251.506432	17.274650
37.039534	1254.002008	17.279667
37.027546	1269.518096	17.284685
37.416873	1255.942601	17.289703
37.407774	1257.288919	17.294720
37.479409	1252.591600	17.299738
37.804713	1261.357760	17.304755
37.613679	1244.596769	17.309773
37.425160	1235.039581	17.314791
37.108195	1229.150591	17.319808
37.226330	1240.905383	17.324826
37.591728	1244.004031	17.329843
37.256697	1248.351645	17.334861
37.688738	1249.621314	17.339879
37.107622	1255.944501	17.344896
37.380900	1261.527406	17.349914
37.264085	1251.043303	17.354931
37.058046	1254.568132	17.359949
37.330912	1254.655149	17.364967
37.226018	1262.829274	17.369984
37.553384	1272.142506	17.375002
37.752939	1270.696557	17.380019
37.762740	1283.799395	17.385037
37.984152	1279.837924	17.390055
37.788125	1282.879834	17.395072
37.800241	1280.233716	17.400090
38.231879	1272.325167	17.405107
38.111861	1287.501439	17.410125
38.176624	1277.306098	17.415143
38.418351	1276.838103	17.420160
38.303614	1269.324998	17.425178
38.105474	1253.535652	17.430195
38.310556	1246.165027	17.435213
38.303398	1236.001634	17.440231
37.758630	1249.672642	17.445248
38.396638	1259.571801	17.450266
38.507286	1254.519060	17.455283
38.490370	1268.933282	17.460301
38.387121	1256.252718	17.465319
38.302170	1246.450924	17.470336
38.324171	1261.876642	17.475354
38.430964	1266.336260	17.480371
38.653210	1269.682680	17.485389
38.421843	1276.083797	17.490407
38.309275	1277.523695	17.495424
38.203534	1275.962849	17.500442
38.597846	1271.978524	17.505459
38.266642	1279.090819	17.510477
38.408002	1267.898588	17.515495
38.432033	1276.575958	17.520512
38.889785	1282.961552	17.525530
38.681287	1285.313344	17.530547
38.858175	1293.733546	17.535565
39.200865	1296.971103	17.540583
39.084989	1298.526357	17.545600
39.176727	1276.836149	17.550618
39.045077	1272.915259	17.555635
38.776568	1269.492808	17.560653
39.292314	1262.676648	17.565671
39.141425	1278.112655	17.570688
38.781560	1268.670858	17.575706
38.719375	1291.696471	17.580723
39.434366	1287.780544	17.585741
39.651731	1299.747639	17.590759
39.420495	1292.482756	17.595776
39.316585	1302.836887	17.600794
39.849611	1293.100092	17.605811
39.069600	1295.977174	17.610829
39.361793	1292.492034	17.615847
39.415906	1295.984820	17.620864
39.472310	1282.542619	17.625882
39.613419	1292.541499	17.630899
39.515566	1287.595929	17.635917
39.588066	1296.279738	17.640935
39.429651	1299.861474	17.645952
39.145648	1291.760320	17.650970
39.683038	1292.546019	17.655987
39.662637	1302.447973	17.661005
39.472800	1288.763476	17.666023
39.246475	1298.539399	17.671040
39.576873	1300.817830	17.676058
39.964144	1319.748140	17.681075
39.908928	1316.299525	17.686093
40.273351	1307.421713	17.691111
39.900839	1306.122053	17.696128
40.243125	1319.768054	17.701146
40.646789	1305.295204	17.706163
40.206279	1304.199864	17.711181
40.118949	1300.446499	17.716199
40.277042	1283.489787	17.721216
40.216897	1283.837547	17.726234
40.639535	1284.680871	17.731251
39.944610	1283.486115	17.736269
40.382864	1293.717593	17.741287
40.866154	1309.157879	17.746304
40.311074	1302.940332	17.751322
40.505216	1280.326181	17.756339
40.298799	1288.088664	17.761357
40.792204	1291.874744	17.766375
40.575371	1298.281419	17.771392
40.611207	1298.867120	17.776410
40.877195	1295.920969	17.781427
40.487200	1303.970706	17.786445
40.623479	1300.480544	17.791463
40.908537	1305.361614	17.796480
40.923779	1317.565446	17.801498
40.974766	1311.106522	17.806515
40.730805	1315.774675	17.811533
41.082019	1311.001288	17.816551
41.128694	1301.283853	17.821568
40.807036	1320.852602	17.826586
41.285361	1303.424810	17.831603
40.764932	1320.595015	17.836621
40.848853	1311.974289	17.841639
41.011403	1309.074519	17.846656
40.986801	1313.098945	17.851674
41.394961	1311.402653	17.856691
41.282602	1310.074085	17.861709
41.128233	1317.313920	17.866727
41.311722	1309.617955	17.871744
41.147246	1316.258525	17.876762
41.282996	1309.897765	17.881779
41.077847	1324.305884	17.886797
41.194824	1304.771304	17.891815
41.302309	1317.979713	17.896832
41.433575	1331.878023	17.901850
41.535644	1332.484622	17.906867
41.843110	1332.795777	17.911885
41.597724	1344.515823	17.916903
41.940635	1340.085088	17.921920
41.448469	1336.462344	17.926938
41.944932	1339.294725	17.931955
41.439710	1334.643764	17.936973
41.447456	1333.722315	17.941991
41.917273	1345.101789	17.947008
41.970776	1343.400711	17.952026
41.976090	1333.924224	17.957043
41.771970	1330.859566	17.962061
42.074577	1326.292121	17.967079
41.814593	1330.753628	17.972096
41.891189	1341.800996	17.977114
42.079017	1331.203756	17.982131
41.961892	1335.872135	17.987149
42.164434	1345.823502	17.992167
42.224969	1348.155992	17.997184
42.225782	1363.860469	18.002202
42.466099	1365.542175	18.007219
42.204863	1369.450205	18.012237
42.435583	1368.534090	18.017255
42.592652	1362.924151	18.022272
42.511741	1360.461164	18.027290
42.787780	1355.756379	18.032307
42.640081	1367.578052	18.037325
42.542020	1359.271817	18.042343
42.815089	1354.172689	18.047360
42.615993	1369.198855	18.052378
42.913004	1366.993335	18.057395
42.470850	1359.808459	18.062413
42.696750	1372.317717	18.067431
42.980189	1355.178127	18.072448
42.434573	1366.432496	18.077466
42.922706	1372.099151	18.082483
42.845700	1375.958924	18.087501
42.447468	1369.551170	18.092519
42.821771	1368.970796	18.097536
42.781685	1387.889131	18.102554
42.999823	1385.229012	18.107571
43.120427	1392.027065	18.112589
43.323087	1387.113755	18.117607
43.444676	1381.403291	18.122624
43.242023	1383.456873	18.127642
43.301116	1385.526910	18.132659
43.246033	1384.324478	18.137677
43.462630	1387.673399	18.142695
43.819398	1385.511827	18.147712
43.365036	1391.923392	18.152730
43.211066	1382.642160	18.157747
43.379499	1386.745928	18.162765
43.467448	1381.817883	18.167783
43.570925	1385.187990	18.172800
43.517049	1385.828901	18.177818
43.712384	1390.790375	18.182835
43.720722	1406.111463	18.187853
43.849019	1413.495023	18.192871
44.158057	1411.433866	18.197888
44.108187	1406.003988	18.202906
44.133606	1400.340314	18.207923
43.498889	1393.578592	18.212941
43.950731	1389.360124	18.217959
43.923783	1406.733292	18.222976
43.809610	1415.494133	18.227994
44.107464	1410.792144	18.233011
43.948609	1405.238079	18.238029
43.998228	1406.974585	18.243047
44.177883	1400.197807	18.248064
44.234965	1411.435525	18.253082
44.687189	1404.195287	18.258099
44.608429	1398.469580	18.263117
44.676244	1404.464398	18.268135
44.733427	1404.533907	18.273152
44.331102	1407.989406	18.278170
44.490036	1403.229352	18.283187
44.504780	1401.499843	18.288205
44.431583	1408.155784	18.293223
44.949715	1400.206631	18.298240
44.544694	1394.281281	18.303258
44.736446	1398.554363	18.308275
44.424273	1400.067004	18.313293
44.241925	1411.747165	18.318311
44.922562	1415.862059	18.323328
44.478360	1425.235524	18.328346
44.806616	1419.762639	18.333363
45.058106	1425.331780	18.338381
44.996649	1428.888647	18.343399
45.029290	1419.627964	18.348416
45.090940	1428.842107	18.353434
44.992943	1422.885082	18.358451
45.207291	1433.319107	18.363469
45.354993	1422.320797	18.368487
45.435232	1433.973254	18.373504
44.848912	1439.559617	18.378522
45.491506	1441.339980	18.383539
45.568261	1457.046603	18.388557
45.261983	1454.520444	18.393575
46.086857	1453.099016	18.398592
45.735789	1459.676603	18.403610
45.721537	1449.243638	18.408627
45.858692	1450.554065	18.413645
45.719562	1440.817407	18.418663
45.811773	1424.537984	18.423680
45.155705	1428.079573	18.428698
45.516584	1438.059233	18.433715
46.127276	1444.113776	18.438733
45.810130	1453.155544	18.443751
46.087178	1443.261277	18.448768
46.307339	1452.233082	18.453786
45.884651	1444.915286	18.458803
46.269377	1450.593746	18.463821
45.939629	1445.677240	18.468839
46.245752	1444.368433	18.473856
45.999484	1450.067304	18.478874
45.992831	1450.154859	18.483891
46.305010	1445.788766	18.488909
46.197956	1452.329007	18.493927
46.288475	1449.631029	18.498944
46.075947	1448.277526	18.503962
46.461912	1436.165281	18.508979
46.384384	1450.606653	18.513997
46.246458	1453.733711	18.519015
46.640449	1445.374907	18.524032
46.313127	1469.833611	18.529050
46.659713	1469.646184	18.534067
47.108296	1465.487989	18.539085
46.826988	1471.639186	18.544103
47.339446	1455.163721	18.549120
46.867125	1452.044284	18.554138
46.614988	1444.600190	18.559155
46.979645	1447.637655	18.564173
46.957452	1459.028049	18.569191
47.279841	1461.230708	18.574208
47.008365	1464.726699	18.579226
47.125272	1468.563436	18.584243
47.266343	1462.719274	18.589261
47.134909	1467.025043	18.594279
47.289645	1471.080686	18.599296
47.048299	1468.095865	18.604314
47.463018	1461.385387	18.609331
47.331088	1462.771763	18.614349
47.251974	1463.699840	18.619367
47.829114	1454.500158	18.624384
47.412021	1468.075503	18.629402
47.554100	1463.152954	18.634419
47.694042	1462.693323	18.639437
47.126166	1464.800444	18.644455
46.911003	1458.868382	18.649472
47.134536	1467.632024	18.654490
47.470837	1481.807659	18.659507
47.737770	1493.364323	18.664525
47.754711	1490.755149	18.669543
47.791495	1494.802868	18.674560
47.561934	1495.994036	18.679578
47.897250	1490.855046	18.684595
48.303084	1490.266494	18.689613
48.163879	1494.104759	18.694631
48.447832	1487.221646	18.699648
48.238040	1489.060880	18.704666
48.116395	1489.552157	18.709683
48.200050	1480.118136	18.714701
48.094858	1500.972346	18.719719
48.276716	1487.193776	18.724736
47.985274	1494.005683	18.729754
48.094501	1498.463412	18.734771
48.460806	1512.475419	18.739789
48.458966	1519.960011	18.744807
48.678131	1513.310584	18.749824
48.976313	1524.041185	18.754842
48.842780	1521.732851	18.759859
49.108214	1509.858414	18.764877
48.976660	1515.568903	18.769895
49.007007	1492.647068	18.774912
48.604165	1495.641782	18.779930
48.618404	1503.246495	18.784947
48.749654	1503.716316	18.789965
48.923315	1525.616175	18.794983
48.942283	1515.037867	18.800000
48.781443	1511.258418	18.805018
49.005882	1511.309117	18.810035
49.063593	1511.804824	18.815053
48.714359	1525.385130	18.820071
48.941930	1510.897690	18.825088
49.325184	1517.594141	18.830106
49.282199	1543.350961	18.835123
49.366546	1542.662671	18.840141
49.264779	1536.290929	18.845159
49.844118	1528.670142	18.850176
49.594271	1544.679055	18.855194
49.971024	1544.091993	18.860211
50.281959	1523.263068	18.865229
49.432858	1518.106900	18.870247
49.842157	1509.827414	18.875264
49.883533	1515.488301	18.880282
49.767676	1526.793014	18.885299
49.600925	1524.623681	18.890317
49.737341	1530.731878	18.895335
49.713634	1530.951139	18.900352
49.597155	1535.853856	18.905370
49.923545	1527.107817	18.910387
50.323297	1528.399967	18.915405
49.848101	1529.619302	18.920423
50.210067	1528.178888	18.925440
50.277187	1529.108815	18.930458
50.435293	1535.408607	18.935475
50.445531	1528.263966	18.940493
50.289941	1537.338221	18.945511
50.264211	1529.604722	18.950528
50.201484	1538.755401	18.955546
50.453826	1563.859554	18.960563
50.473539	1550.929463	18.965581
50.188744	1568.472933	18.970599
50.331809	1569.406481	18.975616
50.587001	1555.916594	18.980634
50.437787	1565.123554	18.985651
50.737730	1556.054532	18.990669
51.132899	1555.725651	18.995687
50.913514	1556.180610	19.000704
51.125441	1565.400760	19.005722
50.875384	1563.361109	19.010739
51.234885	1550.969850	19.015757
50.838553	1558.781640	19.020775
51.304956	1564.368470	19.025792
51.262866	1560.610968	19.030810
50.933981	1556.817409	19.035827
50.915951	1565.572446	19.040845
50.890506	1580.666302	19.045863
50.979978	1584.455536	19.050880
51.705290	1585.816892	19.055898
51.483629	1593.390062	19.060915
51.498790	1582.459958	19.065933
51.461215	1589.000191	19.070951
51.657270	1584.322247	19.075968
52.044497	1582.564771	19.080986
51.591540	1580.681744	19.086003
51.704714	1581.612195	19.091021
51.706856	1578.166954	19.096039
51.605563	1586.988765	19.101056
51.834052	1580.910394	19.106074
51.712828	1585.653438	19.111091
52.020103	1574.050699	19.116109
51.839516	1581.821802	19.121127
51.944069	1604.384025	19.126144
52.434417	1600.629687	19.131162
52.264512	1609.353916	19.136179
52.239201	1608.330758	19.141197
52.461476	1604.323446	19.146215
52.426219	1609.799966	19.151232
52.464376	1605.648986	19.156250
52.389699	1613.316700	19.161267
52.943469	1605.283104	19.166285
52.812532	1603.932303	19.171303
52.688951	1590.210212	19.176320
53.031115	1583.284738	19.181338
52.677386	1575.504425	19.186355
53.147291	1572.123010	19.191373
52.879734	1568.437642	19.196391
52.743476	1565.354244	19.201408
52.745141	1563.854887	19.206426
52.810634	1579.494228	19.211443
53.156208	1585.765717	19.216461
52.851140	1589.946632	19.221479
52.500862	1597.749526	19.226496
53.121696	1590.935333	19.231514
52.957427	1593.567979	19.236531
52.874661	1595.128995	19.241549
52.930188	1591.591867	19.246567
53.212626	1594.364055	19.251584
53.293986	1607.998461	19.256602
53.121239	1623.476072	19.261619
53.528238	1621.149156	19.266637
53.210365	1627.592538	19.271655
53.226081	1618.269934	19.276672
53.328683	1622.978867	19.281690
53.175415	1626.081667	19.286707
53.417995	1617.018610	19.291725
53.505408	1636.173336	19.296743
53.682438	1646.858857	19.301760
53.951228	1649.501099	19.306778
54.016095	1645.279782	19.311795
54.039678	1650.968727	19.316813
54.128332	1649.880201	19.321831
53.886814	1650.809022	19.326848
54.421140	1642.866595	19.331866
54.194204	1647.407869	19.336883
54.214273	1647.404648	19.341901
54.285231	1646.196249	19.346919
54.202021	1641.083056	19.351936
54.554792	1642.574617	19.356954
54.300726	1650.272532	19.361971
54.518263	1635.086579	19.366989
54.419174	1647.911386	19.372007
54.422203	1641.897261	19.377024
54.488024	1641.126978	19.382042
54.290272	1650.418811	19.387059
54.168703	1659.354010	19.392077
54.221614	1667.127246	19.397095
54.476333	1678.849601	19.402112
54.725745	1671.682476	19.407130
54.401280	1689.333090	19.412147
54.811227	1684.993807	19.417165
55.283169	1687.106585	19.422183
55.119123	1697.967661	19.427200
55.360450	1695.706481	19.432218
55.557972	1694.934068	19.437235
55.611901	1685.249826	19.442253
55.864375	1696.706714	19.447271
55.604542	1681.308981	19.452288
55.575048	1662.137051	19.457306
55.449940	1664.192461	19.462323
55.410577	1666.095772	19.467341
55.529826	1659.050084	19.472359
55.583905	1673.623272	19.477376
55.766789	1680.340743	19.482394
55.779640	1693.721889	19.487411
55.841574	1686.600386	19.492429
55.882990	1686.082530	19.497447
56.013324	1691.623906	19.502464
56.193145	1682.171271	19.507482
55.971968	1680.430590	19.512499
56.032341	1679.346571	19.517517
56.362932	1674.054116	19.522535
56.427517	1689.849450	19.527552
56.712473	1691.266889	19.532570
56.495405	1680.851944	19.537587
56.246265	1659.044069	19.542605
56.379473	1666.353044	19.547623
56.302982	1665.747027	19.552640
56.662552	1663.067449	19.557658
56.347962	1681.665006	19.562675
56.512157	1692.215756	19.567693
56.801786	1680.433276	19.572711
56.552998	1696.041068	19.577728
56.783413	1694.402970	19.582746
56.613990	1687.699033	19.587763
56.937862	1687.691405	19.592781
56.741192	1702.683708	19.597799
56.653538	1699.403768	19.602816
56.985204	1696.157629	19.607834
56.683122	1695.801519	19.612851
56.682902	1692.262246	19.617869
57.064744	1698.685303	19.622887
57.085059	1714.225029	19.627904
57.248394	1721.184737	19.632922
57.138860	1721.675663	19.637939
57.058816	1730.126085	19.642957
57.245575	1715.059787	19.647975
57.085898	1721.743820	19.652992
57.430842	1720.417788	19.658010
57.347862	1728.418794	19.663027
57.484658	1736.414642	19.668045
57.857121	1738.689584	19.673063
57.618037	1750.610298	19.678080
57.938855	1742.992878	19.683098
57.971706	1751.779238	19.688115
57.997768	1735.351141	19.693133
57.968233	1749.295947	19.698151
58.238024	1749.212001	19.703168
58.167153	1738.864935	19.708186
58.033628	1748.772649	19.713203
58.114702	1744.482652	19.718221
58.502732	1741.537399	19.723239
58.077970	1744.645770	19.728256
58.280697	1740.890076	19.733274
58.261181	1749.447260	19.738291
58.030227	1749.048344	19.743309
58.098967	1754.876420	19.748327
58.089209	1770.685271	19.753344
58.328214	1768.278158	19.758362
58.670714	1771.883944	19.763379
58.496928	1766.888971	19.768397
59.044612	1774.237293	19.773415
58.641424	1774.035730	19.778432
58.640673	1767.628900	19.783450
58.840725	1770.376509	19.788467
59.221050	1787.678890	19.793485
59.453265	1783.319159	19.798503
59.455525	1776.021512	19.803520
59.587401	1770.663186	19.808538
59.071013	1760.788275	19.813555
59.397521	1759.244957	19.818573
59.343021	1760.820359	19.823591
59.452176	1764.178639	19.828608
59.377354	1754.920723	19.833626
59.556211	1766.523114	19.838643
59.493508	1771.958454	19.843661
59.897378	1782.971269	19.848679
59.784010	1770.903774	19.853696
59.952432	1781.178635	19.858714
59.922920	1777.947607	19.863731
59.703902	1780.271267	19.868749
60.369365	1775.672558	19.873767
59.747948	1776.794106	19.878784
60.099437	1768.009315	19.883802
60.064362	1773.207442	19.888819
60.176651	1771.817836	19.893837
60.427964	1770.355721	19.898855
60.107583	1781.798643	19.903872
60.555619	1765.071982	19.908890
60.633905	1766.232952	19.913907
60.359237	1772.073329	19.918925
60.816767	1758.102675	19.923943
60.352675	1773.044890	19.928960
60.457782	1770.294190	19.933978
60.164713	1766.063853	19.938995
60.410448	1769.379904	19.944013
60.537498	1771.335340	19.949031
60.469799	1780.666289	19.954048
61.155637	1794.171436	19.959066
60.868028	1803.702639	19.964083
60.703226	1804.679009	19.969101
61.141583	1803.844588	19.974119
60.865193	1804.947293	19.979136
61.269996	1797.413979	19.984154
61.251857	1800.212120	19.989171
60.899845	1803.261710	19.994189
61.309098	1798.779359	19.999207
61.204963	1805.775471	20.004224
61.323692	1805.647976	20.009242
61.537515	1825.489083	20.014259
61.346341	1834.591220	20.019277
61.731736	1836.878273	20.024295
61.178400	1836.448969	20.029312
61.470712	1830.410654	20.034330
61.381373	1835.801502	20.039347
61.507347	1833.266113	20.044365
61.952401	1847.998922	20.049383
61.900873	1860.984646	20.054400
62.290913	1858.685568	20.059418
62.377269	1862.311776	20.064435
62.423600	1859.246388	20.069453
62.873288	1849.822966	20.074471
62.948180	1848.782238	20.079488
62.484901	1836.772064	20.084506
62.384109	1831.356439	20.089523
62.312348	1829.700449	20.094541
62.658315	1819.499208	20.099559
62.236195	1823.480204	20.104576
62.782384	1830.669918	20.109594
62.635617	1836.148576	20.114611
62.610935	1852.532480	20.119629
62.766145	1860.794449	20.124647
62.708767	1850.813241	20.129664
62.546542	1852.778641	20.134682
62.843148	1863.498736	20.139699
62.727496	1862.233563	20.144717
62.980723	1855.430684	20.149735
62.894515	1854.851377	20.154752
62.918115	1872.761311	20.159770
63.473026	1859.394807	20.164787
63.545051	1877.389833	20.169805
63.554006	1872.191074	20.174823
63.634570	1876.024277	20.179840
63.558379	1871.285839	20.184858
63.337826	1869.804584	20.189875
63.099480	1880.592702	20.194893
63.467944	1876.708294	20.199911
63.176490	1876.142843	20.204928
63.428868	1888.992036	20.209946
63.666727	1892.008921	20.214963
63.885571	1901.799196	20.219981
63.828307	1895.317951	20.224999
63.944362	1904.141472	20.230016
64.022591	1898.046034	20.235034
64.178642	1897.690788	20.240051
64.310864	1897.937098	20.245069
64.481101	1894.452390	20.250087
64.336509	1902.752756	20.255104
64.337639	1921.652629	20.260122
64.870466	1919.719312	20.265139
64.722790	1922.898362	20.270157
64.534221	1925.597864	20.275175
64.495135	1930.749495	20.280192
64.886542	1932.511783	20.285210
65.018777	1936.412268	20.290227
65.248391	1937.234510	20.295245
65.411169	1909.548174	20.300263
65.160368	1923.286186	20.305280
64.921913	1924.439479	20.310298
65.082473	1919.702594	20.315315
64.909428	1919.693990	20.320333
65.372858	1917.620728	20.325351
65.432348	1920.329434	20.330368
65.231940	1918.928333	20.335386
65.555996	1927.246785	20.340403
65.074982	1928.624379	20.345421
65.206385	1919.094368	20.350439
65.392667	1929.253228	20.355456
65.665016	1953.475536	20.360474
66.197791	1941.834971	20.365491
66.207259	1944.428961	20.370509
65.721934	1933.971670	20.375527
65.846382	1934.978999	20.380544
66.260337	1946.658874	20.385562
66.234139	1938.404554	20.390579
66.123355	1950.572388	20.395597
66.142332	1941.206585	20.400615
66.220629	1944.804212	20.405632
66.131086	1940.704962	20.410650
66.344526	1941.550234	20.415667
66.067550	1953.318279	20.420685
66.458366	1938.842133	20.425703
66.408645	1952.760466	20.430720
66.197347	1948.268494	20.435738
66.473210	1942.684220	20.440755
66.212373	1964.278078	20.445773
66.465864	1966.880348	20.450791
66.436207	1972.436336	20.455808
66.369971	1977.098377	20.460826
66.885635	1969.349091	20.465843
66.861189	1996.393657	20.470861
67.106533	1988.080274	20.475879
67.318610	1988.543515	20.480896
67.355817	1995.633583	20.485914
67.523524	1980.072966	20.490931
67.318104	1989.932534	20.495949
67.552772	1980.655006	20.500967
67.796632	1981.937455	20.505984
67.688699	1989.783706	20.511002
67.609148	1980.337635	20.516019
67.685880	1975.288480	20.521037
67.945746	1982.928206	20.526055
67.776364	1994.502945	20.531072
67.623904	1976.765953	20.536090
67.998495	1984.433003	20.541107
67.799389	1989.622759	20.546125
67.997657	1995.095216	20.551143
68.312907	2010.644855	20.556160
68.476621	2013.377857	20.561178
68.733104	2011.453991	20.566195
68.580087	2019.044748	20.571213
68.765070	2005.469687	20.576231
68.516263	1994.139343	20.581248
68.382269	2004.741020	20.586266
68.584944	1990.069882	20.591283
68.507983	2013.427764	20.596301
68.486628	2011.302811	20.601319
69.183668	2005.453142	20.606336
68.752134	2012.646285	20.611354
68.636630	2012.373669	20.616371
68.657061	2009.376875	20.621389
68.872108	2009.016937	20.626407
68.839709	2013.830899	20.631424
69.041289	2027.754846	20.636442
69.260797	2029.209500	20.641459
69.483505	2031.936243	20.646477
69.479783	2038.598696	20.651495
69.499042	2021.461914	20.656512
69.160503	2028.550570	20.661530
69.261523	2018.534547	20.666547
69.603018	2033.502716	20.671565
69.498050	2022.161995	20.676583
69.882875	2036.368192	20.681600
69.823633	2045.122225	20.686618
70.320477	2049.993373	20.691635
70.385409	2051.806168	20.696653
70.237528	2029.575736	20.701671
70.224616	2031.797352	20.706688
70.190374	2025.935305	20.711706
70.253640	2041.292351	20.716723
70.362748	2050.856405	20.721741
70.422975	2046.330539	20.726759
70.379041	2053.929087	20.731776
70.578781	2064.523205	20.736794
70.594930	2056.995108	20.741811
70.560390	2061.378410	20.746829
70.359132	2056.356256	20.751847
70.631389	2048.902154	20.756864
70.351675	2061.131627	20.761882
70.813906	2068.251480	20.766899
71.012626	2071.822068	20.771917
70.907671	2091.067849	20.776935
71.019034	2087.422594	20.781952
71.177954	2086.406203	20.786970
71.350343	2072.329709	20.791987
71.333846	2083.656762	20.797005
71.337098	2080.977304	20.802023
71.314254	2068.863663	20.807040
71.174617	2080.664966	20.812058
71.548379	2087.153982	20.817075
71.594984	2111.838855	20.822093
71.697527	2103.192668	20.827111
71.945565	2104.277830	20.832128
71.785947	2113.296455	20.837146
71.968731	2100.610435	20.842163
71.794745	2105.686112	20.847181
71.905411	2119.014297	20.852199
72.333286	2103.511162	20.857216
72.135829	2118.436376	20.862234
72.164895	2124.395200	20.867251
72.488399	2144.595215	20.872269
72.441656	2134.409190	20.877287
72.753703	2140.135698	20.882304
72.879310	2139.398328	20.887322
72.906432	2137.282929	20.892339
72.773360	2134.238228	20.897357
72.763418	2136.857371	20.902375
73.180052	2131.044505	20.907392
72.948359	2131.724816	20.912410
73.194972	2133.749326	20.917427
72.940415	2138.461901	20.922445
72.854338	2130.328708	20.927463
73.100048	2136.168043	20.932480
72.725245	2134.521018	20.937498
73.160273	2125.326280	20.942515
72.928153	2143.794867	20.947533
73.011081	2153.849241	20.952551
73.102028	2146.858170	20.957568
73.385257	2158.294790	20.962586
73.452218	2150.914275	20.967603
73.458297	2163.541862	20.972621
73.702131	2179.573419	20.977639
73.883415	2180.184727	20.982656
74.041903	2185.949900	20.987674
74.052160	2184.900578	20.992691
73.869557	2185.887677	20.997709
73.869947	2189.993306	21.002727
74.291351	2179.406967	21.007744
74.134638	2191.363669	21.012762
74.394583	2205.025215	21.017779
74.459618	2194.442212	21.022797
74.439406	2206.499858	21.027815
74.865216	2202.710045	21.032832
74.762769	2202.235563	21.037850
75.139970	2196.183561	21.042867
74.945972	2199.739729	21.047885
75.063661	2207.329887	21.052903
75.198285	2197.830642	21.057920
75.123864	2191.622568	21.062938
75.300833	2188.979883	21.067955
75.277134	2200.199634	21.072973
75.538429	2204.472878	21.077991
75.618892	2198.674269	21.083008
75.322724	2194.189462	21.088026
75.870916	2192.307146	21.093043
75.613745	2199.749434	21.098061
75.190877	2196.228674	21.103079
75.406795	2190.894546	21.108096
75.171583	2201.797234	21.113114
75.732736	2208.438898	21.118131
75.549303	2226.596223	21.123149
75.810888	2221.858861	21.128167
76.139433	2233.212020	21.133184
75.788715	2234.238516	21.138202
76.056664	2219.861127	21.143219
76.095837	2225.200163	21.148237
76.058009	2255.378548	21.153255
76.356205	2246.598039	21.158272
76.664296	2250.985748	21.163290
76.212333	2262.159008	21.168307
76.537857	2253.601446	21.173325
76.451381	2253.413861	21.178343
76.757630	2255.697089	21.183360
76.565860	2286.483699	21.188378
76.998848	2280.399171	21.193395
77.236812	2275.947926	21.198413
77.017376	2284.984062	21.203431
77.330271	2285.769449	21.208448
77.417437	2273.491011	21.213466
77.180722	2276.871532	21.218483
77.349022	2266.552017	21.223501
77.187633	2268.447337	21.228519
77.337684	2271.085036	21.233536
77.296119	2277.538908	21.238554
77.493265	2298.203683	21.243571
77.857362	2294.876735	21.248589
77.698830	2304.685778	21.253607
77.737750	2307.961787	21.258624
77.825573	2299.585255	21.263642
77.667539	2312.314651	21.268659
78.011297	2299.399861	21.273677
77.732946	2309.539485	21.278695
78.495634	2319.395119	21.283712
78.394120	2323.624006	21.288730
78.633491	2332.963758	21.293747
78.768559	2324.022019	21.298765
78.800402	2333.122723	21.303783
79.099467	2321.810149	21.308800
79.028271	2331.528201	21.313818
78.760157	2322.481652	21.318835
79.304534	2319.055161	21.323853
78.878593	2322.620818	21.328871
79.078261	2319.877745	21.333888
78.999896	2334.335859	21.338906
78.963881	2317.685760	21.343923
79.390614	2318.641765	21.348941
79.263453	2318.873602	21.353959
79.401230	2316.849074	21.358976
79.362314	2318.063387	21.363994
79.459911	2318.144547	21.369011
79.446184	2314.254119	21.374029
79.547098	2331.349231	21.379047
79.907011	2327.024035	21.384064
79.433705	2348.476944	21.389082
79.842349	2352.353127	21.394099
79.779843	2340.333678	21.399117
79.974484	2345.208287	21.404135
80.112199	2344.502799	21.409152
80.010338	2362.723579	21.414170
79.921182	2376.389832	21.419187
80.067000	2378.099316	21.424205
80.275726	2383.674078	21.429223
80.434392	2372.040134	21.434240
80.625081	2376.782459	21.439258
80.434468	2398.461719	21.444275
81.009793	2402.030537	21.449293
80.859400	2405.626207	21.454311
81.147170	2399.188819	21.459328
81.320209	2395.166335	21.464346
81.046525	2395.775485	21.469363
81.153272	2393.015755	21.474381
81.243477	2400.624554	21.479399
81.679179	2381.880093	21.484416
81.725156	2398.953370	21.489434
81.476756	2400.435487	21.494451
81.738223	2384.875218	21.499469
81.663303	2399.010363	21.504487
81.890617	2400.912929	21.509504
81.377413	2395.871185	21.514522
81.339507	2389.433038	21.519539
81.768125	2401.014200	21.524557
81.710556	2424.366503	21.529575
82.152289	2423.424544	21.534592
81.868050	2424.106167	21.539610
81.909316	2432.399219	21.544627
82.553348	2421.264375	21.549645
82.423090	2429.857710	21.554663
82.529311	2431.568009	21.559680
82.620690	2430.053469	21.564698
82.847136	2439.398498	21.569715
82.870696	2446.355675	21.574733
82.912065	2453.269116	21.579751
83.338242	2445.292382	21.584768
83.132763	2446.633159	21.589786
83.252517	2442.534999	21.594803
83.233370	2441.957559	21.599821
83.330693	2440.009468	21.604839
83.543245	2436.121464	21.609856
83.209983	2442.504730	21.614874
83.183702	2438.044450	21.619891
83.367233	2436.494764	21.624909
83.102046	2448.712805	21.629927
83.340563	2453.237519	21.634944
83.814877	2472.733578	21.639962
83.725615	2479.209303	21.644979
83.869819	2472.351163	21.649997
83.937484	2468.809527	21.655015
83.866943	2476.307928	21.660032
83.834324	2486.345563	21.665050
84.323685	2492.843072	21.670067
84.325081	2497.873612	21.675085
84.240743	2507.908498	21.680103
84.646540	2497.754664	21.685120
84.658813	2504.672769	21.690138
84.464554	2515.949851	21.695155
84.602611	2502.487996	21.700173
84.586424	2514.568065	21.705191
84.633782	2517.305561	21.710208
85.168810	2524.410886	21.715226
85.179436	2536.272756	21.720243
85.415140	2527.922850	21.725261
85.235339	2544.230803	21.730279
85.069052	2537.614065	21.735296
85.383626	2521.191771	21.740314
85.165990	2534.825176	21.745331
85.482654	2534.829716	21.750349
85.710620	2563.918665	21.755367
85.851147	2555.288177	21.760384
85.981849	2557.870023	21.765402
86.064998	2552.910886	21.770419
86.498652	2542.191766	21.775437
85.989642	2550.358693	21.780455
85.858341	2548.282656	21.785472
86.161002	2557.260871	21.790490
86.304353	2546.800411	21.795507
86.090975	2546.633845	21.800525
86.434863	2544.575631	21.805543
86.577273	2546.563333	21.810560
86.576530	2542.589759	21.815578
86.507216	2555.574220	21.820595
86.760444	2568.430961	21.825613
86.446123	2564.471991	21.830631
86.463619	2573.272309	21.835648
86.910906	2573.735818	21.840666
86.833952	2578.702584	21.845683
87.279596	2592.677822	21.850701
87.514808	2599.773577	21.855719
87.301097	2589.087652	21.860736
87.509119	2588.399257	21.865754
87.856914	2588.999762	21.870771
87.874009	2584.939170	21.875789
87.766922	2590.254471	21.880807
87.653536	2583.071606	21.885824
87.788535	2585.268933	21.890842
87.729367	2600.022354	21.895859
88.218061	2603.878762	21.900877
88.167856	2623.418553	21.905895
88.317225	2609.965806	21.910912
88.673649	2626.882872	21.915930
88.249653	2620.108193	21.920947
88.523950	2614.517623	21.925965
88.687388	2607.914343	21.930983
88.355169	2613.921541	21.936000
88.687563	2623.166419	21.941018
88.898986	2629.573811	21.946035
89.187318	2635.783314	21.951053
89.165123	2636.148649	21.956071
89.140585	2641.289560	21.961088
89.222351	2637.203696	21.966106
88.818215	2635.846022	21.971123
89.157074	2632.847087	21.976141
88.973206	2634.493552	21.981159
89.393461	2658.784695	21.986176
89.421499	2665.082912	21.991194
89.506561	2665.799254	21.996211
89.672888	2665.841141	22.001229
89.495659	2664.772916	22.006247
89.870499	2675.834306	22.011264
90.278640	2684.197207	22.016282
90.268674	2686.851061	22.021299
90.401644	2690.902654	22.026317
90.553253	2705.897867	22.031335
90.275622	2696.538762	22.036352
90.783940	2702.515000	22.041370
90.308853	2691.095916	22.046387
90.512268	2694.946715	22.051405
90.733465	2702.469499	22.056423
90.796823	2688.315411	22.061440
91.265721	2684.222073	22.066458
90.650743	2698.626897	22.071475
90.942548	2686.109400	22.076493
91.160137	2700.324042	22.081511
91.197396	2719.592022	22.086528
91.639629	2724.064672	22.091546
91.394137	2734.580833	22.096563
91.562037	2728.569856	22.101581
91.604599	2726.333139	22.106599
91.481120	2730.763860	22.111616
91.691175	2713.536845	22.116634
91.596075	2732.523122	22.121651
91.782638	2730.071519	22.126669
91.991986	2744.529780	22.131687
91.842100	2751.010574	22.136704
91.929687	2743.005871	22.141722
92.054868	2749.065249	22.146739
92.495952	2758.957529	22.151757
92.410515	2774.322543	22.156775
92.784307	2773.514104	22.161792
92.903574	2777.515206	22.166810
92.558058	2777.937609	22.171827
92.743074	2769.261359	22.176845
93.265952	2766.660945	22.181863
92.907384	2762.366820	22.186880
92.874453	2769.203377	22.191898
93.014333	2783.605896	22.196915
93.399478	2791.314169	22.201933
93.531930	2786.359677	22.206951
93.721802	2785.021316	22.211968
93.619321	2787.025293	22.216986
93.924401	2793.590868	22.222003
93.714144	2789.899978	22.227021
93.517271	2790.422956	22.232039
93.225116	2806.734173	22.237056
94.109473	2814.843446	22.242074
94.082574	2821.111163	22.247091
94.331240	2821.312179	22.252109
94.451363	2833.813615	22.257127
94.299358	2831.253951	22.262144
94.713245	2817.463870	22.267162
94.401566	2826.614942	22.272179
94.763855	2833.447498	22.277197
94.820787	2849.851759	22.282215
95.021617	2849.057526	22.287232
95.264616	2846.825796	22.292250
95.249635	2846.055752	22.297267
95.132943	2845.097418	22.302285
95.509496	2843.792210	22.307303
95.266284	2845.945273	22.312320
95.286709	2841.737777	22.317338
95.097944	2850.789820	22.322355
95.277273	2854.409318	22.327373
95.726490	2855.668541	22.332391
95.626438	2873.582908	22.337408
95.837699	2872.906569	22.342426
95.781713	2875.485993	22.347443
96.304119	2885.865652	22.352461
96.275330	2875.402517	22.357479
95.947931	2880.200880	22.362496
96.495426	2878.284774	22.367514
96.021137	2881.543642	22.372531
95.941010	2891.310685	22.377549
96.325389	2897.744104	22.382567
96.326388	2907.050660	22.387584
96.542104	2904.524375	22.392602
96.774002	2919.116864	22.397619
97.167477	2928.916958	22.402637
97.421853	2935.170547	22.407655
97.340208	2937.437870	22.412672
97.644986	2932.229315	22.417690
97.153920	2936.409590	22.422707
97.423102	2936.148763	22.427725
97.721479	2924.717849	22.432743
97.441968	2924.306973	22.437760
97.914142	2918.960821	22.442778
97.931327	2931.909799	22.447795
97.917363	2936.946873	22.452813
98.165438	2928.257327	22.457831
98.078199	2946.347505	22.462848
98.532586	2933.667008	22.467866
98.885480	2942.506095	22.472883
98.270515	2942.140844	22.477901
98.715029	2933.397946	22.482919
98.258420	2933.124644	22.487936
98.696980	2924.830262	22.492954
98.360333	2941.182546	22.497971
98.397409	2955.832883	22.502989
98.775887	2961.422488	22.508007
99.061392	2969.499919	22.513024
99.315898	2963.315362	22.518042
99.530441	2958.899897	22.523059
99.191838	2963.516801	22.528077
99.835989	2965.801323	22.533095
99.347628	2994.037871	22.538112
99.771973	2985.243885	22.543130
99.768480	3000.131989	22.548147
99.506337	2994.217797	22.553165
100.291707	2976.027203	22.558183
100.142973	2979.523640	22.563200
100.114973	2989.906979	22.568218
99.903083	2986.225738	22.573235
99.911920	3002.027455	22.578253
100.266936	3011.331113	22.583271
100.424309	3018.837497	22.588288
100.658171	3018.218901	22.593306
100.830795	3028.334302	22.598323
100.892467	3016.741270	22.603341
101.062329	3016.348403	22.608359
100.765781	3019.695372	22.613376
101.122180	3020.785352	22.618394
101.250416	3032.026351	22.623411
101.306265	3046.400841	22.628429
101.608427	3037.822166	22.633447
101.321653	3047.177848	22.638464
101.707725	3035.151580	22.643482
101.621443	3049.339507	22.648499
101.401366	3039.689406	22.653517
101.813155	3048.705587	22.658535
101.765094	3066.216249	22.663552
102.094506	3061.662876	22.668570
102.290040	3067.685998	22.673587
102.176621	3071.555171	22.678605
102.378927	3063.643694	22.683623
102.397678	3054.627241	22.688640
102.479051	3084.215702	22.693658
103.131158	3086.717646	22.698675
103.151782	3087.109202	22.703693
103.309748	3087.598417	22.708711
102.728701	3106.840436	22.713728
103.303667	3080.490991	22.718746
103.432294	3077.671010	22.723763
103.164737	3092.195439	22.728781
103.185313	3085.311891	22.733799
102.943144	3082.187635	22.738816
103.176014	3107.572870	22.743834
103.674381	3111.558449	22.748851
103.694184	3114.419226	22.753869
104.169355	3105.791685	22.758887
103.949739	3117.479937	22.763904
104.150995	3125.859567	22.768922
104.149620	3124.068710	22.773939
104.125092	3140.212555	22.778957
104.346713	3139.781542	22.783975
104.427837	3145.255025	22.788992
104.533612	3139.097257	22.794010
104.756899	3142.265396	22.799027
104.783521	3145.816501	22.804045
104.781576	3154.686343	22.809063
104.761036	3164.787806	22.814080
105.023949	3177.724562	22.819098
105.491371	3173.497607	22.824115
105.377817	3170.218316	22.829133
105.881722	3163.377221	22.834151
105.840246	3167.234947	22.839168
105.993831	3158.446277	22.844186
105.829947	3161.618739	22.849203
105.784465	3158.073741	22.854221
106.173748	3160.796951	22.859239
105.866528	3163.149834	22.864256
106.069399	3164.188795	22.869274
106.370625	3168.067387	22.874291
106.130185	3192.931225	22.879309
106.500313	3189.163416	22.884327
106.477319	3184.612713	22.889344
106.786477	3188.720515	22.894362
106.683577	3186.443996	22.899379
106.566626	3177.288641	22.904397
106.883485	3175.851339	22.909415
106.925159	3208.034258	22.914432
106.667760	3216.954312	22.919450
106.827508	3209.851078	22.924467
106.884366	3221.478022	22.929485
107.385235	3226.592779	22.934503
107.460197	3245.081435	22.939520
107.818607	3238.252494	22.944538
108.004519	3240.498437	22.949555
107.889130	3246.120496	22.954573
108.191954	3239.010166	22.959591
108.242352	3239.605424	22.964608
108.361143	3240.674317	22.969626
108.504239	3233.086828	22.974643
108.419014	3249.341943	22.979661
108.683554	3264.723246	22.984679
108.788389	3263.669779	22.989696
108.655554	3261.431844	22.994714
108.973912	3262.630955	22.999731
109.040926	3264.994185	23.004749
109.155470	3257.803746	23.009767
109.355045	3257.719986	23.014784
109.242293	3261.795189	23.019802
109.218591	3261.990090	23.024819
109.498358	3284.920280	23.029837
109.674963	3273.103417	23.034855
109.949691	3286.524501	23.039872
109.754486	3289.381054	23.044890
109.602097	3289.825373	23.049907
109.360063	3293.827596	23.054925
110.301822	3300.864521	23.059943
110.496795	3320.005101	23.064960
110.234019	3319.914047	23.069978
110.945046	3317.709875	23.074995
110.681482	3312.688565	23.080013
110.687653	3309.260363	23.085031
110.808895	3316.417907	23.090048
111.002781	3301.688648	23.095066
111.114271	3306.475372	23.100083
111.102324	3307.230028	23.105101
111.684547	3320.153752	23.110119
111.769227	3325.147699	23.115136
111.600760	3343.825537	23.120154
111.615511	3332.297158	23.125171
111.487842	3333.250399	23.130189
111.553877	3335.874947	23.135207
111.734177	3330.709699	23.140224
111.515314	3322.867602	23.145242
111.776412	3325.103929	23.150259
111.503676	3353.572655	23.155277
111.725957	3361.957721	23.160295
112.385598	3361.688903	23.165312
112.253865	3360.225577	23.170330
112.677081	3375.251324	23.175347
112.688676	3389.327223	23.180365
112.851083	3378.206320	23.185383
112.707227	3396.335187	23.190400
112.865693	3383.838359	23.195418
113.182920	3384.316349	23.200435
112.707974	3404.400018	23.205453
113.215007	3406.334418	23.210471
113.110104	3416.882137	23.215488
113.182738	3410.734259	23.220506
113.843402	3429.748025	23.225523
113.869006	3432.394769	23.230541
114.090706	3446.567010	23.235559
114.014979	3444.751785	23.240576
114.040704	3436.192574	23.245594
114.258662	3432.763610	23.250611
114.224141	3438.327225	23.255629
114.531541	3452.476366	23.260647
114.667891	3446.545642	23.265664
114.627071	3466.550733	23.270682
114.620295	3460.694741	23.275699
114.644894	3461.191077	23.280717
115.077807	3462.761308	23.285735
115.333977	3477.374086	23.290752
115.294190	3495.814496	23.295770
115.658681	3492.053017	23.300787
115.445000	3499.620389	23.305805
115.497887	3489.100527	23.310823
116.157052	3488.357462	23.315840
116.029458	3487.965605	23.320858
116.019612	3483.087057	23.325875
115.765261	3494.709567	23.330893
116.511246	3516.746925	23.335911
116.683507	3511.523901	23.340928
116.333907	3524.161398	23.345946
116.618409	3521.572125	23.350963
116.507402	3529.116061	23.355981
116.610376	3525.992522	23.360999
116.795683	3519.375120	23.366016
116.387232	3535.446110	23.371034
116.652580	3544.731374	23.376051
117.062286	3543.505776	23.381069
117.225670	3546.834586	23.386087
117.411648	3555.124867	23.391104
117.210279	3575.877814	23.396122
117.898367	3566.845563	23.401139
117.704761	3569.710567	23.406157
118.038986	3577.521775	23.411175
118.127443	3567.000905	23.416192
118.288332	3576.561640	23.421210
118.503623	3561.263135	23.426227
118.773432	3556.445376	23.431245
118.814657	3555.023673	23.436263
118.641299	3556.602486	23.441280
118.584034	3554.980957	23.446298
118.727380	3561.728420	23.451315
118.854563	3559.896559	23.456333
118.734537	3578.653499	23.461351
118.873979	3575.394344	23.466368
118.909785	3582.182563	23.471386
119.073464	3589.968270	23.476403
119.448495	3608.223113	23.481421
119.273112	3615.317976	23.486439
119.622980	3615.358921	23.491456
119.354283	3621.761503	23.496474
120.188828	3618.657377	23.501491
120.023789	3635.800360	23.506509
120.038073	3648.252509	23.511527
120.371583	3636.334820	23.516544
120.115462	3644.502140	23.521562
120.440738	3634.038640	23.526579
120.694131	3650.425061	23.531597
120.455872	3671.947042	23.536615
121.135025	3677.704516	23.541632
121.002941	3677.983566	23.546650
121.135291	3658.526765	23.551667
120.991322	3678.039653	23.556685
121.625041	3681.598705	23.561703
121.839508	3679.804828	23.566720
122.065738	3692.033645	23.571738
122.479140	3681.559994	23.576755
122.306535	3677.091201	23.581773
122.519552	3672.596320	23.586791
122.335105	3676.271670	23.591808
122.392543	3671.108589	23.596826
122.499010	3665.148717	23.601843
123.024519	3682.017243	23.606861
122.942777	3683.184221	23.611879
123.100192	3671.071970	23.616896
122.791766	3684.991515	23.621914
123.120381	3668.253414	23.626931
123.113678	3672.083703	23.631949
122.819360	3674.425954	23.636967
122.990804	3674.128787	23.641984
122.962095	3695.379045	23.647002
123.411318	3693.102509	23.652019
123.725581	3706.686801	23.657037
123.452363	3700.328859	23.662055
123.950567	3710.805794	23.667072
123.855320	3723.859930	23.672090
124.167516	3714.854489	23.677107
124.022468	3729.872101	23.682125
124.190904	3721.887010	23.687143
124.327960	3719.801051	23.692160
124.369546	3732.532101	23.697178
124.536012	3752.029413	23.702195
124.392906	3753.081109	23.707213
124.247350	3751.719847	23.712231
124.752927	3754.705453	23.717248
124.682144	3779.686398	23.722266
125.150395	3785.334380	23.727283
125.163930	3792.798023	23.732301
125.246507	3807.116297	23.737319
125.489264	3807.786315	23.742336
125.647329	3821.641832	23.747354
125.954498	3801.887941	23.752371
126.546441	3813.662090	23.757389
126.365429	3830.496345	23.762407
126.467074	3833.072828	23.767424
126.636866	3837.736370	23.772442
126.648426	3831.044272	23.777459
126.994504	3825.832752	23.782477
127.076901	3824.501999	23.787495
127.311039	3817.413357	23.792512
127.056224	3818.681884	23.797530
127.069153	3825.840431	23.802547
127.259055	3823.307095	23.807565
127.268342	3828.632605	23.812583
127.410563	3838.325495	23.817600
127.618064	3845.874657	23.822618
127.773802	3838.762321	23.827635
128.013853	3841.090188	23.832653
127.949830	3837.452801	23.837671
128.074029	3859.754231	23.842688
128.645885	3866.456322	23.847706
128.446503	3876.823567	23.852723
128.793110	3867.142341	23.857741
128.373036	3878.719995	23.862759
128.899657	3875.568163	23.867776
128.861017	3886.141052	23.872794
128.688342	3902.589400	23.877811
129.229606	3902.975838	23.882829
129.269740	3903.211698	23.887847
129.385169	3898.381474	23.892864
129.623923	3918.602978	23.897882
129.635063	3923.571098	23.902899
129.710768	3931.157052	23.907917
129.564180	3925.226412	23.912935
130.123377	3922.946467	23.917952
130.040133	3947.205200	23.922970
130.023711	3954.737418	23.927987
130.415880	3954.424718	23.933005
130.500826	3960.259748	23.938023
130.562546	3969.436945	23.943040
130.567860	3977.107303	23.948058
130.963383	3982.741002	23.953075
131.279278	3975.506307	23.958093
131.101374	3991.297964	23.963111
131.623288	3969.571345	23.968128
131.739768	3974.175782	23.973146
131.802320	3975.968746	23.978163
131.877046	3980.140116	23.983181
131.885382	3985.682159	23.988199
132.224295	4009.721863	23.993216
132.235148	4011.452277	23.998234
132.254534	4021.076772	24.003251
132.610560	4008.164821	24.008269
132.645861	4012.049072	24.013287
132.712684	4009.822450	24.018304
132.512543	4013.981019	24.023322
132.523789	4018.790255	24.028339
133.095230	4026.150113	24.033357
133.046638	4039.552649	24.038375
133.128957	4033.444658	24.043392
133.138527	4042.018215	24.048410
133.178933	4058.992846	24.053427
133.796145	4065.605203	24.058445
133.342216	4069.655579	24.063463
133.869451	4061.930895	24.068480
134.005506	4082.202040	24.073498
134.005347	4090.815721	24.078515
134.296514	4092.885329	24.083533
133.987080	4100.943405	24.088551
134.372361	4106.185466	24.093568
134.803410	4125.380712	24.098586
134.789971	4134.517291	24.103603
135.446823	4119.055764	24.108621
135.217792	4125.332669	24.113639
135.133937	4129.688268	24.118656
135.557101	4126.535575	24.123674
135.832108	4137.171911	24.128691
136.200751	4140.681310	24.133709
136.024447	4134.440666	24.138727
136.092802	4138.468355	24.143744
136.375758	4143.187110	24.148762
136.377730	4136.323340	24.153779
136.483814	4130.961187	24.158797
136.084797	4136.320447	24.163815
136.486056	4136.962062	24.168832
136.604710	4144.404404	24.173850
136.652748	4160.842234	24.178867
136.767957	4153.903763	24.183885
136.534840	4166.367481	24.188903
137.178563	4185.511590	24.193920
136.923019	4189.080407	24.198938
136.864831	4197.418638	24.203955
137.255708	4200.321152	24.208973
137.487600	4223.612868	24.213991
137.725069	4221.306301	24.219008
138.310117	4227.686295	24.224026
138.533315	4251.904537	24.229043
138.644347	4241.499155	24.234061
138.821648	4243.384772	24.239079
139.188602	4244.566782	24.244096
139.160164	4232.328734	24.249114
138.827860	4237.045716	24.254131
139.507904	4228.124481	24.259149
139.193230	4235.526617	24.264167
139.515701	4228.159381	24.269184
139.663735	4226.615959	24.274202
139.289742	4232.020035	24.279219
139.967320	4224.390080	24.284237
139.536162	4238.005617	24.289255
139.779067	4227.468301	24.294272
139.997607	4251.397801	24.299290
139.864607	4259.161945	24.304307
140.511768	4255.971937	24.309325
140.369806	4263.838203	24.314343
140.654640	4286.550473	24.319360
140.567277	4283.966871	24.324378
140.682166	4287.319317	24.329395
140.945243	4284.196050	24.334413
140.835219	4300.022054	24.339431
140.977044	4316.462412	24.344448
141.037169	4320.715658	24.349466
141.025895	4330.246913	24.354483
141.547182	4340.155811	24.359501
141.545997	4346.649782	24.364519
142.083311	4355.553941	24.369536
142.047011	4368.703089	24.374554
142.285517	4377.088515	24.379571
142.327306	4382.173048	24.384589
141.889444	4387.559044	24.389607
142.806875	4401.195703	24.394624
142.864797	4408.787100	24.399642
142.825260	4409.689382	24.404659
143.004118	4405.549788	24.409677
143.263499	4421.510540	24.414695
143.337134	4431.020455	24.419712
143.945692	4433.669619	24.424730
143.812832	4433.865419	24.429747
144.310649	4421.773795	24.434765
144.351118	4430.084629	24.439783
144.173077	4421.557331	24.444800
144.715140	4426.957802	24.449818
144.618404	4436.122011	24.454835
144.919694	4435.140191	24.459853
145.053985	4448.303116	24.464871
144.946215	4447.233119	24.469888
145.340790	4444.569500	24.474906
145.059761	4446.300878	24.479923
145.405252	4437.153598	24.484941
145.488999	4439.918693	24.489959
145.541134	4448.930162	24.494976
146.158903	4456.015392	24.499994
145.621333	4472.797887	24.505011
145.859946	4472.455384	24.510029
145.993479	4475.743542	24.515047
146.195973	4481.125803	24.520064
146.353117	4474.365359	24.525082
146.379545	4474.549923	24.530099
146.803048	4501.567037	24.535117
146.580124	4501.010205	24.540135
146.778094	4500.997499	24.545152
147.044423	4496.641761	24.550170
147.052128	4511.719202	24.555187
147.244279	4521.748355	24.560205
147.104570	4533.540629	24.565223
147.551939	4537.876942	24.570240
147.554336	4526.693364	24.575258
147.699081	4554.649456	24.580275
148.114814	4553.017691	24.585293
148.132494	4559.105978	24.590311
148.275143	4576.763464	24.595328
148.517683	4575.378004	24.600346
148.414420	4585.850780	24.605363
148.549975	4588.529764	24.610381
148.787263	4607.354553	24.615399
149.339234	4603.899599	24.620416
149.466922	4612.372056	24.625434
149.609099	4609.919357	24.630451
149.577859	4597.023012	24.635469
149.769746	4606.234135	24.640487
149.903816	4622.189913	24.645504
150.091305	4618.463456	24.650522
149.921947	4623.720192	24.655539
150.083204	4636.462054	24.660557
150.571378	4637.793905	24.665575
150.580766	4651.545688	24.670592
150.634896	4651.412743	24.675610
150.609133	4658.394572	24.680627
150.864925	4679.817228	24.685645
151.149508	4685.795358	24.690663
151.298407	4685.411302	24.695680
151.710626	4680.545302	24.700698
151.863860	4683.396124	24.705715
151.929358	4696.666215	24.710733
151.874207	4716.322081	24.715751
152.184388	4705.571524	24.720768
152.665922	4702.274099	24.725786
152.348283	4704.319718	24.730803
152.654017	4702.758184	24.735821
152.832831	4726.884381	24.740839
152.842497	4724.289163	24.745856
152.959604	4734.098359	24.750874
153.236510	4733.339891	24.755891
153.295359	4738.308547	24.760909
153.163496	4755.356291	24.765927
153.536401	4753.709308	24.770944
153.682220	4756.772156	24.775962
153.510212	4757.459578	24.780979
154.186094	4773.340149	24.785997
154.448243	4776.566175	24.791015
154.783578	4779.169287	24.796032
154.886735	4778.263090	24.801050
155.020072	4781.862872	24.806067
155.129579	4775.012339	24.811085
154.989308	4782.743304	24.816103
155.106230	4770.782927	24.821120
155.336102	4777.586386	24.826138
155.161720	4775.741883	24.831155
155.701741	4800.234629	24.836173
155.904123	4796.008574	24.841191
155.734901	4808.398140	24.846208
155.706988	4801.484543	24.851226
155.682007	4815.854780	24.856243
155.959258	4828.059109	24.861261
156.195740	4835.875568	24.866279
156.258028	4846.663553	24.871296
156.987449	4856.181682	24.876314
156.790872	4859.783737	24.881331
156.852812	4864.973786	24.886349
157.304834	4863.536021	24.891367
157.321696	4895.370238	24.896384
157.669314	4885.500171	24.901402
158.248171	4889.147735	24.906419
158.032685	4878.515478	24.911437
158.046484	4886.811942	24.916455
158.351172	4879.504647	24.921472
158.649029	4898.476704	24.926490
158.620057	4912.769003	24.931507
158.702994	4915.550839	24.936525
158.906942	4906.509226	24.941543
158.839234	4914.556736	24.946560
158.984273	4912.684102	24.951578
159.146599	4936.075366	24.956595
159.533585	4929.049931	24.961613
159.818208	4938.672073	24.966631
159.709395	4937.938905	24.971648
160.273085	4937.624807	24.976666
160.299978	4955.487648	24.981683
160.285650	4956.167246	24.986701
160.724898	4959.400478	24.991719
160.335285	4954.073792	24.996736
160.492973	4962.443333	25.001754
160.809851	4979.557461	25.006771
161.192343	4984.248035	25.011789
161.224187	4982.356466	25.016807
161.017053	4986.017662	25.021824
161.620556	4989.101990	25.026842
161.739943	5005.271358	25.031859
161.904581	5003.113955	25.036877
162.291275	5008.792731	25.041895
162.090841	5003.525547	25.046912
162.288445	5012.680160	25.051930
162.560422	5018.193145	25.056947
162.752778	5036.526104	25.061965
162.888118	5033.426982	25.066983
162.769641	5036.304674	25.072000
162.995143	5036.273420	25.077018
163.086825	5039.285958	25.082035
163.368502	5044.809208	25.087053
163.406236	5054.822439	25.092071
163.605826	5064.647813	25.097088
163.732771	5063.242979	25.102106
163.963074	5068.191492	25.107123
164.057326	5090.590826	25.112141
164.193791	5083.340146	25.117159
164.339363	5083.117883	25.122176
164.482696	5094.867052	25.127194
164.531390	5118.906863	25.132211
164.770949	5123.311101	25.137229
165.007398	5116.499959	25.142247
165.374843	5134.205665	25.147264
165.769634	5143.561783	25.152282
165.726262	5150.264229	25.157299
165.751151	5145.435446	25.162317
165.860599	5149.714897	25.167335
166.091118	5165.368746	25.172352
166.530084	5171.510484	25.177370
166.671425	5167.902958	25.182387
166.548983	5181.683336	25.187405
166.685402	5164.701986	25.192423
166.694360	5196.264344	25.197440
167.032316	5197.395206	25.202458
167.227508	5196.738641	25.207475
167.259799	5202.749342	25.212493
167.647137	5218.505691	25.217511
167.933193	5227.210505	25.222528
168.122882	5221.416104	25.227546
167.833642	5224.484691	25.232563
167.862808	5252.385016	25.237581
168.469441	5247.099994	25.242599
168.345854	5257.711800	25.247616
168.836628	5272.362923	25.252634
169.176715	5288.653183	25.257651
169.117248	5269.504113	25.262669
169.145775	5283.668813	25.267687
169.582567	5290.669239	25.272704
169.721805	5297.603824	25.277722
169.841890	5313.954362	25.282739
169.696870	5308.026842	25.287757
170.126786	5302.168935	25.292775
170.079528	5320.882667	25.297792
170.443323	5328.212577	25.302810
170.698861	5335.381169	25.307827
170.914046	5325.269952	25.312845
171.142196	5335.951609	25.317863
171.111843	5357.233641	25.322880
171.648632	5357.321114	25.327898
171.642026	5354.877066	25.332915
171.297341	5368.422424	25.337933
171.653819	5358.662343	25.342951
171.880682	5362.719381	25.347968
171.716365	5371.322223	25.352986
171.797347	5377.079780	25.358003
172.089940	5388.147700	25.363021
173.050312	5400.770691	25.368039
172.673503	5400.491674	25.373056
173.089551	5399.731446	25.378074
173.191649	5393.100512	25.383091
173.047891	5410.987180	25.388109
173.169007	5413.527011	25.393127
173.684858	5426.971414	25.398144
173.746971	5431.911464	25.403162
173.976024	5441.232833	25.408179
173.590895	5465.810468	25.413197
174.271707	5465.806537	25.418215
174.376500	5482.051134	25.423232
174.556288	5492.497522	25.428250
174.868114	5489.138087	25.433267
174.912813	5495.958030	25.438285
175.322301	5489.218256	25.443303
175.675712	5520.882163	25.448320
175.805446	5514.043796	25.453338
175.866680	5517.866882	25.458355
175.833543	5520.085170	25.463373
176.381799	5512.630953	25.468391
176.577064	5515.562565	25.473408
176.500035	5527.916793	25.478426
176.863633	5535.573326	25.483443
176.608415	5544.655710	25.488461
176.614336	5536.709710	25.493479
176.874765	5553.640763	25.498496
177.082885	5559.150761	25.503514
177.448937	5567.994075	25.508531
177.201672	5574.826773	25.513549
177.866300	5583.444696	25.518567
177.973201	5596.499732	25.523584
177.957873	5588.889087	25.528602
178.709834	5599.980698	25.533619
178.633694	5615.888465	25.538637
178.961709	5613.747410	25.543655
178.969661	5610.076864	25.548672
179.264767	5618.587724	25.553690
179.569647	5622.093493	25.558707
179.313341	5641.394024	25.563725
179.809253	5638.522870	25.568743
179.786700	5640.633281	25.573760
179.785086	5642.878031	25.578778
180.222371	5656.539719	25.583795
180.197224	5672.383560	25.588813
180.375699	5670.127875	25.593831
180.494257	5676.554566	25.598848
180.831570	5687.291454	25.603866
181.401106	5703.996388	25.608883
180.835358	5701.983651	25.613901
181.596774	5700.000064	25.618919
181.301347	5703.820269	25.623936
181.462872	5703.964428	25.628954
181.906441	5711.790825	25.633971
181.817636	5729.729695	25.638989
182.050884	5730.266011	25.644007
182.129504	5733.485323	25.649024
181.957270	5752.839466	25.654042
182.494332	5755.032182	25.659059
182.617125	5775.876584	25.664077
183.192305	5781.591701	25.669095
183.464412	5788.200871	25.674112
183.065504	5788.273887	25.679130
183.887369	5801.333916	25.684148
184.077708	5800.715864	25.689165
184.106472	5797.373167	25.694183
184.327033	5798.756454	25.699200
184.646111	5791.798086	25.704218
184.845849	5810.027773	25.709236
184.681462	5827.291210	25.714253
185.179956	5815.637344	25.719271
184.916947	5836.500856	25.724288
184.819243	5837.283474	25.729306
185.507992	5841.274876	25.734324
185.346698	5858.751848	25.739341
185.512036	5851.902929	25.744359
185.887336	5876.181424	25.749376
186.379250	5880.631415	25.754394
186.469268	5873.936893	25.759412
186.360602	5901.131118	25.764429
186.843998	5889.079154	25.769447
187.101775	5900.257649	25.774464
187.290474	5898.455032	25.779482
187.715943	5908.001861	25.784500
187.879394	5921.172474	25.789517
187.657344	5927.761360	25.794535
187.757089	5923.487624	25.799552
188.157966	5927.404575	25.804570
188.409209	5931.331221	25.809588
188.461076	5959.160031	25.814605
188.552322	5945.704849	25.819623
188.635737	5953.920796	25.824640
188.579150	5972.057016	25.829658
189.280313	5971.975108	25.834676
189.783829	5987.052903	25.839693
189.601340	5986.390432	25.844711
189.870072	5992.008155	25.849728
190.043953	6010.213889	25.854746
190.348513	6008.115855	25.859764
190.344515	6012.747224	25.864781
190.502832	6012.869084	25.869799
190.648195	6024.039632	25.874816
190.387698	6037.403027	25.879834
191.000761	6042.144517	25.884852
191.097296	6051.317465	25.889869
191.373562	6067.583363	25.894887
191.384926	6073.449061	25.899904
191.501421	6073.212540	25.904922
192.304221	6080.927581	25.909940
192.029660	6088.634218	25.914957
192.154447	6097.893953	25.919975
192.689465	6093.445353	25.924992
192.328702	6110.435956	25.930010
192.763169	6112.501111	25.935028
192.974317	6122.042911	25.940045
192.977703	6128.966503	25.945063
193.265840	6133.380612	25.950080
193.182540	6144.193545	25.955098
194.012198	6149.221533	25.960116
194.085407	6175.356628	25.965133
194.477049	6168.786973	25.970151
194.971309	6156.251572	25.975168
194.734705	6162.813772	25.980186
195.466519	6176.394375	25.985204
195.362809	6196.070182	25.990221
195.296184	6191.420077	25.995239
195.605829	6200.020220	26.000256
195.849709	6197.965665	26.005274
196.192076	6182.726796	26.010292
195.794547	6196.581870	26.015309
196.098235	6201.953355	26.020327
196.409891	6209.961548	26.025344
196.083962	6218.275945	26.030362
196.719412	6228.356756	26.035380
196.809171	6251.479236	26.040397
197.215272	6248.751315	26.045415
197.138936	6260.038421	26.050432
197.522636	6277.771241	26.055450
197.561991	6274.317389	26.060468
197.499282	6302.950293	26.065485
197.664826	6310.518435	26.070503
198.425722	6324.180296	26.075520
198.093062	6341.460930	26.080538
198.629821	6338.088266	26.085556
198.718229	6351.004515	26.090573
198.864428	6356.020374	26.095591
199.233360	6365.498626	26.100608
199.491958	6387.727395	26.105626
200.130256	6386.164602	26.110644
200.005834	6391.870333	26.115661
200.548043	6396.185797	26.120679
200.671982	6392.036312	26.125696
200.521823	6410.999923	26.130714
201.045615	6408.905438	26.135732
201.154548	6428.719168	26.140749
200.935962	6426.348862	26.145767
201.121803	6427.681886	26.150784
201.192393	6449.213751	26.155802
201.716604	6446.488996	26.160820
201.721080	6455.439269	26.165837
201.692389	6472.972928	26.170855
202.308686	6479.025585	26.175872
202.196849	6492.622175	26.180890
202.841202	6480.681760	26.185908
202.962385	6502.772895	26.190925
203.174583	6508.298337	26.195943
203.461348	6505.021351	26.200960
203.433279	6506.903816	26.205978
203.607256	6507.835128	26.210996
203.494666	6532.375801	26.216013
203.663858	6520.947760	26.221031
204.502856	6537.665763	26.226048
204.551527	6549.514583	26.231066
204.792388	6556.963057	26.236084
205.115317	6550.373505	26.241101
204.886727	6550.894575	26.246119
205.192483	6576.453584	26.251136
205.051947	6591.858905	26.256154
205.691221	6586.409291	26.261172
205.907054	6606.044929	26.266189
205.897364	6613.172246	26.271207
206.295352	6606.846074	26.276224
206.526523	6638.787573	26.281242
206.735839	6635.205836	26.286260
207.077557	6644.279485	26.291277
207.183425	6649.135077	26.296295
207.699964	6645.815137	26.301312
207.583823	6663.476257	26.306330
207.870931	6654.791682	26.311348
208.037101	6661.431511	26.316365
207.971999	6690.008110	26.321383
208.581986	6682.379828	26.326400
208.571265	6691.068309	26.331418
208.890112	6696.807346	26.336436
208.902310	6711.217561	26.341453
209.136614	6716.356396	26.346471
209.319097	6719.120345	26.351488
209.393924	6731.788898	26.356506
209.497978	6752.879208	26.361524
209.672981	6746.139274	26.366541
209.986339	6768.778453	26.371559
210.434468	6768.620448	26.376576
210.547816	6794.015384	26.381594
210.576185	6796.181572	26.386612
210.915741	6808.546776	26.391629
211.016171	6820.420606	26.396647
211.694034	6833.767308	26.401664
211.817685	6834.972597	26.406682
211.819161	6837.438908	26.411700
212.315574	6848.705968	26.416717
212.138784	6862.649996	26.421735
212.695951	6860.312522	26.426752
212.910437	6883.234359	26.431770
213.160997	6878.462662	26.436788
213.478338	6879.146910	26.441805
213.637288	6872.223797	26.446823
213.848378	6873.326244	26.451840
213.576048	6872.681198	26.456858
214.005200	6882.909435	26.461876
214.154420	6896.858959	26.466893
213.927964	6908.830605	26.471911
214.552896	6912.919820	26.476928
214.425808	6929.998419	26.481946
214.759825	6939.740676	26.486964
215.383425	6942.177067	26.491981
215.489309	6970.308377	26.496999
215.780741	6957.550507	26.502016
215.718913	6968.904290	26.507034
215.980106	6970.094746	26.512052
216.509148	6983.429903	26.517069
216.321433	6993.080699	26.522087
216.601226	6996.733999	26.527104
216.666668	7013.824490	26.532122
217.041834	7012.710360	26.537140
217.212811	7028.020052	26.542157
217.322664	7029.302303	26.547175
218.318012	7033.577197	26.552192
218.148467	7061.046832	26.557210
218.707809	7059.130705	26.562228
219.112427	7075.914637	26.567245
219.049542	7075.384111	26.572263
219.200524	7085.447545	26.577280
219.117902	7086.629088	26.582298
219.198373	7082.177130	26.587316
219.294971	7097.416138	26.592333
219.125895	7104.561231	26.597351
219.884489	7109.649673	26.602368
219.937504	7121.055290	26.607386
220.068349	7132.211682	26.612404
220.360037	7146.049036	26.617421
220.571952	7160.626910	26.622439
221.105809	7175.277792	26.627456
221.327419	7181.297673	26.632474
221.200355	7192.201747	26.637492
221.384105	7210.232717	26.642509
221.572774	7214.681108	26.647527
222.190276	7236.215055	26.652544
222.269355	7244.905283	26.657562
222.688378	7244.784175	26.662580
223.203906	7256.574875	26.667597
222.883684	7272.075636	26.672615
223.266985	7273.373329	26.677632
223.737900	7282.890208	26.682650
223.903067	7294.759607	26.687668
224.295817	7296.454707	26.692685
224.131977	7298.107136	26.697703
224.625626	7294.023568	26.702720
224.844595	7319.990316	26.707738
224.610501	7327.570757	26.712756
225.294363	7316.001839	26.717773
225.163242	7319.563362	26.722791
225.144475	7339.217702	26.727808
225.412723	7343.231715	26.732826
225.671658	7347.871943	26.737844
225.806015	7379.459886	26.742861
226.062693	7377.714711	26.747879
226.445531	7390.760394	26.752896
226.300451	7420.372431	26.757914
226.326955	7409.434609	26.762932
226.964695	7426.082640	26.767949
227.102654	7438.729931	26.772967
227.244137	7461.974307	26.777984
227.804347	7467.385623	26.783002
228.168460	7474.486025	26.788020
228.488808	7484.154501	26.793037
228.409805	7498.231458	26.798055
228.855217	7497.385418	26.803072
229.144852	7518.040448	26.808090
229.437071	7538.459049	26.813108
229.646953	7531.625865	26.818125
229.590553	7539.649393	26.823143
229.816461	7544.084866	26.828160
230.050843	7558.971920	26.833178
230.304599	7566.571494	26.838196
230.666064	7570.339385	26.843213
230.545446	7593.528968	26.848231
231.280330	7590.513142	26.853248
231.299866	7614.651358	26.858266
231.295618	7612.305701	26.863284
231.615921	7614.699287	26.868301
231.919766	7626.093635	26.873319
232.241266	7636.482759	26.878336
232.229758	7653.717653	26.883354
232.984649	7652.277002	26.888372
233.242025	7669.111046	26.893389
233.221741	7677.576596	26.898407
233.699782	7681.257479	26.903424
233.934389	7686.007914	26.908442
233.635975	7694.171605	26.913460
234.382975	7697.343028	26.918477
234.574496	7714.662867	26.923495
234.727455	7713.177319	26.928512
235.288947	7731.406790	26.933530
235.338394	7732.293514	26.938548
235.701243	7731.534586	26.943565
235.434784	7745.215981	26.948583
235.771639	7753.194248	26.953600
235.910400	7768.319429	26.958618
235.765657	7777.793138	26.963636
236.163946	7784.635670	26.968653
236.305818	7803.630041	26.973671
236.510858	7822.538831	26.978688
236.434376	7829.110857	26.983706
236.823325	7852.561103	26.988724
237.643853	7863.269767	26.993741
237.896454	7862.835274	26.998759
238.177632	7871.817831	27.003776
238.647705	7886.373366	27.008794
238.607376	7884.753376	27.013812
239.140979	7880.289536	27.018829
239.070221	7885.544292	27.023847
239.474566	7888.129105	27.028864
239.594126	7911.512229	27.033882
239.574294	7910.712005	27.038900
239.820958	7908.243687	27.043917
239.929176	7932.874615	27.048935
240.010675	7944.046567	27.053952
240.473109	7960.379296	27.058970
240.532793	7977.633904	27.063988
241.012708	7971.160340	27.069005
241.236560	8002.035049	27.074023
241.297832	8002.171615	27.079040
241.661469	8017.409130	27.084058
241.870538	8027.773963	27.089076
242.403378	8019.582123	27.094093
242.253228	8054.402007	27.099111
242.372023	8055.654597	27.104128
242.944733	8059.390516	27.109146
242.916314	8077.729398	27.114164
243.733579	8090.990504	27.119181
243.766068	8102.863602	27.124199
243.686224	8114.525642	27.129216
244.017485	8122.430249	27.134234
244.124941	8140.866365	27.139252
245.029653	8149.149329	27.144269
244.950073	8167.765581	27.149287
245.457961	8170.426790	27.154304
246.075505	8160.197583	27.159322
245.600838	8204.878472	27.164340
246.075002	8192.435852	27.169357
246.360612	8197.183830	27.174375
246.728185	8199.121472	27.179392
246.639031	8219.982641	27.184410
246.862492	8231.849794	27.189428
247.266859	8243.021650	27.194445
247.025253	8263.149436	27.199463
247.388443	8263.149750	27.204480
247.982777	8272.163680	27.209498
248.140701	8279.118722	27.214516
248.355455	8298.051749	27.219533
248.684253	8323.193851	27.224551
249.018121	8311.229876	27.229568
249.254064	8336.068909	27.234586
249.499189	8342.091024	27.239604
250.162651	8332.203749	27.244621
249.997194	8349.744111	27.249639
250.160190	8369.861055	27.254656
250.598585	8358.918256	27.259674
250.538608	8378.480604	27.264692
250.993687	8386.397879	27.269709
251.093500	8394.354476	27.274727
251.251701	8416.835207	27.279744
251.047439	8409.795381	27.284762
251.341453	8434.931413	27.289780
251.872092	8432.585349	27.294797
252.007234	8445.866590	27.299815
252.357948	8462.339647	27.304832
252.676913	8480.326214	27.309850
252.776477	8486.210282	27.314868
253.033614	8486.303829	27.319885
253.565464	8510.335081	27.324903
253.409041	8517.859677	27.329920
253.876002	8529.859793	27.334938
254.236103	8534.570040	27.339956
254.805247	8546.242280	27.344973
254.962705	8567.402982	27.349991
254.907928	8571.726918	27.355008
255.558982	8564.742681	27.360026
255.333541	8598.364833	27.365044
255.729696	8602.403657	27.370061
256.305347	8612.809614	27.375079
256.404466	8624.277494	27.380096
256.665971	8623.893498	27.385114
256.763271	8639.343285	27.390132
257.156982	8655.675147	27.395149
257.308407	8663.911660	27.400167
257.606496	8689.025439	27.405184
258.129630	8678.472573	27.410202
258.023227	8702.161282	27.415220
258.505406	8715.653414	27.420237
258.344732	8727.157275	27.425255
258.628059	8742.763222	27.430272
259.028143	8731.054327	27.435290
259.041176	8773.640818	27.440308
259.071410	8774.223782	27.445325
259.562339	8802.666627	27.450343
259.723306	8822.198667	27.455360
260.498153	8837.359677	27.460378
260.507785	8845.862434	27.465396
260.835365	8866.769426	27.470413
261.254095	8873.414845	27.475431
261.648624	8887.302353	27.480448
262.002491	8888.002525	27.485466
261.999234	8896.415692	27.490484
262.606990	8907.268809	27.495501
262.833578	8920.570914	27.500519
262.604012	8929.771656	27.505536
263.348727	8928.079142	27.510554
263.206663	8950.614834	27.515572
263.680394	8953.640066	27.520589
263.673399	8977.525828	27.525607
263.859500	8977.377322	27.530624
264.375358	8993.828188	27.535642
264.459797	9018.964381	27.540660
264.563416	9007.682991	27.545677
265.061666	9027.516824	27.550695
265.189167	9037.683687	27.555712
265.401416	9032.255635	27.560730
265.657059	9059.174870	27.565748
266.263909	9064.069045	27.570765
266.605140	9075.352711	27.575783
266.736441	9094.477892	27.580800
267.115195	9084.469473	27.585818
267.149485	9107.114212	27.590836
267.238806	9115.046898	27.595853
268.005455	9135.342107	27.600871
267.673989	9148.095971	27.605888
267.925905	9146.337194	27.610906
268.574086	9169.556589	27.615924
268.682906	9174.924817	27.620941
269.151150	9192.424570	27.625959
269.185928	9209.425680	27.630976
269.536228	9208.205198	27.635994
269.760858	9226.947793	27.641012
269.971567	9242.257370	27.646029
270.603738	9239.473221	27.651047
270.832465	9258.141626	27.656064
271.189865	9265.792049	27.661082
271.517972	9274.906475	27.666100
271.837658	9286.972386	27.671117
272.069110	9300.288219	27.676135
272.216022	9294.543918	27.681152
272.464829	9310.996781	27.686170
272.767944	9323.648860	27.691188
272.932348	9324.511062	27.696205
273.260950	9345.146684	27.701223
272.957728	9356.780375	27.706240
273.586993	9365.779574	27.711258
274.012323	9374.750691	27.716276
274.262863	9399.620646	27.721293
274.512601	9418.348463	27.726311
274.377885	9415.018814	27.731328
275.243243	9421.939933	27.736346
275.310795	9437.113964	27.741364
275.390960	9461.380066	27.746381
275.935094	9469.396654	27.751399
275.833672	9489.198415	27.756416
276.352466	9496.367997	27.761434
276.473023	9506.036197	27.766452
276.925873	9534.641534	27.771469
277.063730	9548.757860	27.776487
277.524310	9557.069925	27.781504
277.910242	9571.796735	27.786522
277.929689	9585.052182	27.791540
278.397018	9586.823417	27.796557
278.760496	9611.048934	27.801575
279.005377	9619.980104	27.806592
279.218787	9629.995966	27.811610
279.554911	9639.259248	27.816628
279.767044	9659.795042	27.821645
279.905957	9660.051061	27.826663
279.940225	9669.247188	27.831680
280.716892	9673.254778	27.836698
280.675285	9683.361685	27.841716
280.697206	9707.585532	27.846733
281.070862	9723.758869	27.851751
281.226340	9738.162551	27.856768
281.610908	9743.936374	27.861786
281.904393	9761.400910	27.866804
282.248491	9784.347087	27.871821
282.630375	9791.739699	27.876839
282.682640	9808.006453	27.881856
283.155950	9821.590323	27.886874
283.348633	9847.078156	27.891892
283.671347	9852.147336	27.896909
284.281771	9872.606170	27.901927
284.379435	9875.275242	27.906944
284.822137	9887.415287	27.911962
284.905728	9905.276226	27.916980
285.038506	9917.289022	27.921997
285.208235	9924.825293	27.927015
285.198203	9949.634997	27.932032
285.974974	9957.212641	27.937050
286.401314	9970.850170	27.942068
286.622877	9986.926843	27.947085
287.126921	9990.759202	27.952103
287.322875	10016.206274	27.957120
287.540135	10025.314825	27.962138
287.512483	10044.935186	27.967156
288.166511	10047.186275	27.972173
288.648435	10069.825260	27.977191
288.755345	10083.018022	27.982208
289.000688	10091.280096	27.987226
289.606177	10106.991155	27.992244
289.982755	10107.738531	27.997261
290.156116	10122.046478	28.002279
290.444380	10131.508926	28.007296
290.531687	10133.933772	28.012314
291.089894	10145.254888	28.017332
291.059394	10166.737412	28.022349
290.985085	10177.330303	28.027367
291.255053	10189.988401	28.032384
291.604159	10204.158635	28.037402
292.184032	10218.226784	28.042420
292.218450	10252.956649	28.047437
292.514824	10253.818729	28.052455
292.720866	10275.032339	28.057472
293.059318	10295.541396	28.062490
293.527803	10309.135137	28.067508
293.912101	10317.828089	28.072525
294.457499	10325.275570	28.077543
294.515266	10350.385196	28.082560
294.829881	10345.693881	28.087578
295.235510	10362.546691	28.092596
295.051323	10376.494773	28.097613
295.294384	10387.007323	28.102631
295.605499	10399.886082	28.107648
296.151989	10408.142438	28.112666
296.444685	10435.440714	28.117684
296.891179	10439.446054	28.122701
297.509999	10444.827499	28.127719
297.411053	10463.308032	28.132736
297.795615	10461.806949	28.137754
298.165469	10477.685019	28.142772
298.106126	10488.901389	28.147789
298.740196	10492.036751	28.152807
298.632962	10502.221561	28.157824
299.027868	10510.810629	28.162842
299.481927	10531.576240	28.167860
299.622046	10548.437342	28.172877
300.426913	10563.866848	28.177895
300.744097	10585.967426	28.182912
300.650891	10581.029393	28.187930
300.843651	10586.817590	28.192948
301.058407	10614.476066	28.197965
301.136687	10634.269582	28.202983
301.312279	10648.899946	28.208000
301.911039	10662.629463	28.213018
302.145027	10693.042222	28.218036
302.567567	10711.292779	28.223053
302.927616	10716.290986	28.228071
303.163011	10739.667942	28.233088
303.544571	10759.912632	28.238106
304.150191	10762.039338	28.243124
304.312502	10778.400570	28.248141
304.763823	10786.173352	28.253159
305.204977	10801.992397	28.258176
305.137070	10815.139687	28.263194
305.478110	10818.286802	28.268212
305.511237	10845.168375	28.273229
306.094160	10846.126875	28.278247
306.424192	10862.276524	28.283264
306.360291	10880.392719	28.288282
306.812022	10894.915173	28.293300
307.019755	10912.376618	28.298317
307.806387	10926.068567	28.303335
308.184522	10945.390903	28.308352
308.575010	10970.531565	28.313370
308.816632	10974.677523	28.318388
309.009635	10981.343735	28.323405
309.406613	10988.069128	28.328423
309.962346	11006.943767	28.333440
309.641268	11016.065135	28.338458
310.066877	11027.251049	28.343476
309.975131	11042.169949	28.348493
310.257249	11061.012711	28.353511
310.576242	11079.184598	28.358528
310.666067	11101.123056	28.363546
311.174552	11111.862971	28.368564
311.180228	11144.768498	28.373581
311.865383	11157.693757	28.378599
312.007078	11175.866866	28.383616
312.382700	11197.790217	28.388634
313.108684	11210.197456	28.393652
312.875734	11240.338468	28.398669
313.594306	11246.805739	28.403687
313.436520	11259.967741	28.408704
313.771232	11291.135752	28.413722
314.292423	11297.362981	28.418740
314.660174	11314.048573	28.423757
315.288337	11325.032827	28.428775
315.996789	11345.627590	28.433792
316.091465	11349.182015	28.438810
316.743604	11358.196493	28.443828
316.423263	11383.348031	28.448845
316.885714	11386.589250	28.453863
317.379097	11403.075085	28.458880
317.525313	11407.049451	28.463898
318.031578	11415.061326	28.468916
318.011013	11436.206442	28.473933
318.440882	11458.154976	28.478951
318.773883	11460.041513	28.483968
318.856293	11482.183580	28.488986
319.797512	11499.748785	28.494004
319.734203	11523.094286	28.499021
319.988029	11521.047672	28.504039
320.309573	11534.166970	28.509056
320.690320	11561.857005	28.514074
320.738250	11576.133596	28.519092
321.167921	11591.036837	28.524109
321.687857	11605.344876	28.529127
322.003216	11618.028035	28.534144
321.976891	11650.353422	28.539162
322.565232	11646.896236	28.544180
323.066359	11674.990720	28.549197
323.336371	11680.325895	28.554215
323.786186	11697.843328	28.559232
324.024592	11705.678858	28.564250
324.639100	11720.248579	28.569268
324.777085	11741.612838	28.574285
324.940997	11747.004297	28.579303
325.423312	11764.358433	28.584320
325.331375	11779.551194	28.589338
326.100522	11781.877877	28.594356
325.794230	11805.338092	28.599373
326.211652	11811.837473	28.604391
326.666179	11843.085912	28.609408
326.857483	11852.370107	28.614426
327.303696	11882.724687	28.619444
327.370398	11900.460429	28.624461
327.953670	11913.309316	28.629479
328.529820	11921.002589	28.634496
328.450933	11948.317573	28.639514
329.068700	11960.434160	28.644532
329.211302	11979.719805	28.649549
329.485423	11984.983993	28.654567
329.811617	12007.041542	28.659584
329.996457	12028.580155	28.664602
330.680781	12031.877064	28.669620
330.661187	12058.910083	28.674637
331.094336	12062.461107	28.679655
331.532270	12075.939134	28.684672
331.818054	12101.572772	28.689690
332.537510	12110.542940	28.694708
332.641580	12130.553308	28.699725
333.056577	12140.760871	28.704743
333.135273	12158.731714	28.709760
333.355582	12163.341832	28.714778
334.152187	12187.935763	28.719796
334.332301	12204.375594	28.724813
334.526793	12213.753953	28.729831
334.945650	12225.482948	28.734848
335.135752	12264.823933	28.739866
335.559372	12259.525346	28.744884
335.875579	12283.244032	28.749901
336.077797	12300.549763	28.754919
336.499088	12324.549674	28.759936
336.790245	12350.647447	28.764954
337.036294	12356.754866	28.769972
337.148589	12382.713551	28.774989
338.026920	12395.164402	28.780007
338.126344	12413.634201	28.785024
338.539175	12427.150585	28.790042
339.162332	12455.713689	28.795060
339.337114	12469.201735	28.800077
339.637963	12480.625065	28.805095
340.062630	12500.753070	28.810112
340.395038	12512.212717	28.815130
340.732903	12523.994207	28.820148
340.517164	12548.846081	28.825165
340.877225	12563.805063	28.830183
341.663145	12585.029281	28.835200
341.518466	12622.452699	28.840218
342.217252	12638.285949	28.845236
342.722436	12662.807854	28.850253
342.942303	12675.476032	28.855271
343.524948	12685.702310	28.860288
343.887670	12717.501624	28.865306
343.995538	12724.411222	28.870324
344.209303	12758.597606	28.875341
344.522099	12767.888191	28.880359
345.291411	12772.593024	28.885376
345.385832	12790.064075	28.890394
345.644843	12815.821254	28.895412
346.240341	12833.585982	28.900429
346.216574	12849.764629	28.905447
346.869385	12869.038973	28.910464
346.963867	12888.872216	28.915482
347.486487	12894.368279	28.920500
347.651560	12917.676777	28.925517
347.598005	12939.724578	28.930535
348.283356	12948.972041	28.935552
348.464282	12974.028619	28.940570
348.976973	12995.805625	28.945588
349.410584	13012.247653	28.950605
349.764820	13026.255228	28.955623
350.410243	13039.573542	28.960640
350.319483	13062.775252	28.965658
350.528659	13080.619150	28.970676
350.949903	13097.402094	28.975693
351.116147	13117.716144	28.980711
351.978867	13128.198574	28.985728
352.031562	13165.952178	28.990746
352.439881	13182.694575	28.995764
352.861010	13205.796826	29.000781
353.514290	13219.504261	29.005799
353.879001	13232.383205	29.010816
354.073075	13254.712752	29.015834
354.340690	13271.142552	29.020852
354.908330	13289.458715	29.025869
354.799405	13294.778303	29.030887
355.675499	13320.619240	29.035904
355.743321	13341.591960	29.040922
356.288674	13359.327713	29.045940
356.635707	13373.236203	29.050957
356.801022	13386.380632	29.055975
357.711260	13415.730420	29.060992
357.611570	13429.140857	29.066010
358.273866	13441.495951	29.071028
358.195006	13462.612250	29.076045
358.680462	13474.175558	29.081063
359.041955	13496.861328	29.086080
359.172684	13519.465638	29.091098
359.619829	13539.998197	29.096116
360.136888	13553.998813	29.101133
360.365502	13587.820450	29.106151
360.657994	13602.165651	29.111168
360.680641	13626.553485	29.116186
361.294632	13647.084396	29.121204
361.845697	13666.020382	29.126221
361.890230	13706.332672	29.131239
362.566878	13717.839034	29.136256
362.917388	13741.229446	29.141274
363.074986	13759.945565	29.146292
363.597890	13782.291870	29.151309
364.088361	13810.831449	29.156327
364.516467	13822.195174	29.161344
364.288868	13839.190862	29.166362
364.895530	13854.901633	29.171380
365.212066	13885.600576	29.176397
365.529875	13916.826575	29.181415
366.397542	13919.962558	29.186432
366.842714	13943.523572	29.191450
367.149771	13953.005605	29.196468
367.864160	13963.820529	29.201485
368.002723	13972.116513	29.206503
368.498764	13988.561659	29.211520
368.690430	14002.302729	29.216538
369.015306	14003.199958	29.221556
369.396146	14010.118005	29.226573
369.687718	14038.162408	29.231591
370.211581	14054.188752	29.236608
370.003715	14064.587496	29.241626
370.346776	14077.208779	29.246644
370.732788	14108.203332	29.251661
370.968350	14120.483720	29.256679
371.562534	14136.739818	29.261696
371.520248	14167.473385	29.266714
371.963459	14191.580111	29.271732
372.500900	14207.910367	29.276749
372.779327	14238.702094	29.281767
373.262562	14254.943724	29.286784
373.727213	14277.254091	29.291802
374.194206	14299.701577	29.296820
374.638591	14318.361171	29.301837
374.835610	14342.416350	29.306855
375.574506	14352.983625	29.311872
375.469561	14389.064387	29.316890
375.989482	14409.873158	29.321908
376.982469	14431.873839	29.326925
376.406094	14448.331556	29.331943
377.358969	14466.067923	29.336960
378.144679	14487.955691	29.341978
378.087097	14508.727031	29.346996
378.327097	14530.258632	29.352013
378.484548	14546.772705	29.357031
379.075454	14570.504034	29.362048
379.604958	14602.589196	29.367066
380.166633	14621.525965	29.372084
380.612348	14627.156446	29.377101
380.720868	14658.902422	29.382119
381.308619	14657.974715	29.387136
381.482990	14684.450723	29.392154
381.733186	14707.727046	29.397172
382.466248	14725.966633	29.402189
382.423489	14752.505893	29.407207
383.249087	14766.779546	29.412224
383.593602	14791.980723	29.417242
383.937048	14811.438794	29.422260
384.306894	14820.353830	29.427277
384.772150	14841.811013	29.432295
385.121226	14844.152202	29.437312
385.612460	14877.803589	29.442330
385.626068	14893.804870	29.447348
386.114995	14903.952538	29.452365
386.159436	14935.833259	29.457383
386.637117	14961.795587	29.462400
386.891139	14987.882651	29.467418
387.190357	15005.634164	29.472436
388.099514	14997.678576	29.477453
387.800777	15053.664617	29.482471
388.626252	15054.678557	29.487488
388.747774	15072.873422	29.492506
389.282039	15105.172613	29.497524
389.516952	15134.445881	29.502541
389.924527	15141.454064	29.507559
390.523337	15169.248291	29.512576
390.656347	15194.587746	29.517594
391.025449	15218.162657	29.522612
391.779008	15229.977238	29.527629
391.733838	15281.032106	29.532647
392.157580	15288.103809	29.537664
392.751256	15291.780787	29.542682
393.251692	15342.221677	29.547700
393.424569	15337.847039	29.552717
393.639952	15384.449112	29.557735
394.229379	15408.075313	29.562752
394.768294	15411.272077	29.567770
394.944591	15444.679584	29.572788
395.409240	15478.164911	29.577805
395.745696	15505.807698	29.582823
396.181976	15523.363699	29.587840
396.719487	15560.613285	29.592858
397.196925	15579.640046	29.597876
397.897947	15596.237108	29.602893
398.042986	15627.912948	29.607911
398.531055	15650.480498	29.612928
399.155613	15666.331606	29.617946
399.355959	15689.088829	29.622964
399.897577	15710.316900	29.627981
400.126165	15744.296337	29.632999
400.493040	15756.557317	29.638016
400.655641	15780.042498	29.643034
401.031029	15791.683863	29.648052
401.551073	15825.969730	29.653069
401.712482	15856.173926	29.658087
402.601296	15874.287931	29.663104
402.818549	15897.215964	29.668122
403.341566	15927.009402	29.673140
404.014788	15942.814469	29.678157
404.160129	15971.591300	29.683175
404.566365	15980.700298	29.688192
404.970490	16007.739515	29.693210
404.940594	16025.829049	29.698228
405.826689	16054.235296	29.703245
406.120673	16081.213859	29.708263
406.528965	16101.948649	29.713280
406.703646	16136.604752	29.718298
406.967616	16163.642071	29.723316
407.391848	16177.415452	29.728333
407.871976	16218.207771	29.733351
408.352516	16231.373902	29.738368
409.171092	16251.633845	29.743386
409.338250	16270.688369	29.748404
409.834800	16290.294471	29.753421
409.942872	16308.032486	29.758439
410.600799	16333.562189	29.763456
411.149672	16350.010721	29.768474
411.450496	16369.099573	29.773492
412.186699	16380.389160	29.778509
412.703248	16386.895985	29.783527
412.840285	16406.174341	29.788544
413.005563	16408.442913	29.793562
413.386263	16442.781196	29.798580
413.906180	16454.014958	29.803597
413.780924	16492.597128	29.808615
414.087266	16505.792235	29.813632
414.862493	16532.862607	29.818650
415.041676	16579.131206	29.823668
415.572453	16584.970982	29.828685
415.754830	16626.402294	29.833703
416.041863	16649.216802	29.838720
416.553673	16685.027249	29.843738
416.564044	16712.081238	29.848756
417.808076	16748.278645	29.853773
418.356376	16776.691340	29.858791
418.496682	16792.253794	29.863808
419.363167	16821.053615	29.868826
419.494920	16849.576706	29.873844
419.924768	16867.181823	29.878861
420.310260	16894.292884	29.883879
420.674512	16917.985342	29.888896
421.042473	16936.059203	29.893914
421.252057	16960.835694	29.898932
421.870084	16997.801857	29.903949
422.206777	17032.564561	29.908967
422.357708	17049.223294	29.913984
423.194631	17081.111046	29.919002
423.385838	17116.549805	29.924020
423.920630	17138.457151	29.929037
424.557741	17169.855127	29.934055
425.078849	17197.770228	29.939072
425.876848	17214.996648	29.944090
426.232429	17237.119678	29.949108
427.083167	17255.481133	29.954125
426.971126	17287.530152	29.959143
427.205762	17307.515670	29.964160
427.741292	17324.646052	29.969178
428.237457	17357.224437	29.974196
428.469766	17377.055902	29.979213
428.969878	17408.568310	29.984231
429.560974	17427.464603	29.989248
429.884146	17445.911915	29.994266
430.008588	17467.115489	29.999284
430.706239	17490.324445	30.004301
431.052032	17534.664006	30.009319
431.530831	17551.829269	30.014336
432.046347	17568.617666	30.019354
432.274634	17598.236122	30.024372
432.894643	17618.777134	30.029389
433.546369	17623.190271	30.034407
433.580740	17650.721374	30.039424
434.073385	17677.617741	30.044442
434.249531	17697.840626	30.049460
434.694027	17717.886935	30.054477
435.073750	17748.897600	30.059495
435.177724	17759.374825	30.064512
436.187818	17792.999147	30.069530
436.307701	17818.664874	30.074548
436.900870	17850.434208	30.079565
437.101365	17877.973892	30.084583
437.552594	17913.617722	30.089600
437.852008	17928.803038	30.094618
438.113224	17971.168652	30.099636
438.880529	17995.734134	30.104653
439.402746	18028.199356	30.109671
439.593212	18058.662869	30.114688
440.404390	18083.074657	30.119706
440.502717	18116.848885	30.124724
440.939151	18151.599200	30.129741
441.327430	18174.588409	30.134759
441.777174	18210.050094	30.139776
442.403446	18246.960066	30.144794
442.331302	18283.621565	30.149812
443.386950	18301.115039	30.154829
443.635195	18343.504995	30.159847
443.869129	18378.109738	30.164864
444.639083	18397.488164	30.169882
445.059721	18445.142150	30.174900
445.560649	18473.066513	30.179917
446.193529	18493.854669	30.184935
446.491797	18529.226652	30.189952
447.387063	18561.374903	30.194970
447.453119	18581.428688	30.199988
448.541934	18596.624721	30.205005
448.635921	18633.302309	30.210023
449.104688	18669.454136	30.215040
449.491138	18684.202315	30.220058
450.017357	18706.990025	30.225076
450.644027	18739.675925	30.230093
450.981698	18763.254385	30.235111
451.196171	18791.756850	30.240128
451.792777	18815.971699	30.245146
451.956805	18850.911076	30.250164
452.725157	18861.739504	30.255181
453.193747	18900.639554	30.260199
453.505400	18928.038982	30.265216
454.225674	18946.641752	30.270234
454.472251	18971.946875	30.275252
454.567292	18994.755275	30.280269
455.159443	19031.885549	30.285287
455.791705	19054.910425	30.290304
456.173754	19078.813797	30.295322
456.431229	19103.578804	30.300340
456.706984	19132.575291	30.305357
457.449984	19146.246217	30.310375
457.678178	19178.537459	30.315392
458.457838	19205.441939	30.320410
458.631281	19227.360211	30.325428
458.901760	19248.392949	30.330445
459.541772	19289.178535	30.335463
459.979434	19307.433837	30.340480
460.480875	19337.128636	30.345498
460.677206	19371.039193	30.350516
461.587685	19396.257350	30.355533
462.011980	19429.865171	30.360551
462.150259	19454.717839	30.365568
462.720878	19486.455144	30.370586
462.628699	19512.934458	30.375604
463.541716	19545.381153	30.380621
464.279955	19589.661111	30.385639
464.404228	19614.860379	30.390656
465.121394	19645.636816	30.395674
465.345077	19684.786123	30.400692
466.152345	19716.602741	30.405709
466.809530	19738.793902	30.410727
466.655116	19769.911417	30.415744
467.315936	19797.651658	30.420762
467.713590	19837.266973	30.425780
468.252324	19879.283317	30.430797
468.661927	19900.798352	30.435815
469.074680	19932.281774	30.440832
469.944992	19963.183273	30.445850
470.536015	19998.450536	30.450868
471.035889	20031.812164	30.455885
471.567182	20058.104881	30.460903
471.822372	20085.151530	30.465920
472.106619	20109.933164	30.470938
473.085795	20146.641420	30.475956
473.316203	20171.939649	30.480973
473.816192	20185.493897	30.485991
474.156541	20225.992637	30.491008
474.664844	20241.694237	30.496026
475.112799	20286.195271	30.501044
475.427846	20319.591289	30.506061
476.178306	20341.779479	30.511079
476.559281	20379.688418	30.516096
477.097031	20412.199461	30.521114
477.566977	20438.134443	30.526132
478.034651	20469.970870	30.531149
478.640773	20499.614592	30.536167
478.720874	20531.580611	30.541184
479.833165	20559.517249	30.546202
479.971523	20603.933452	30.551220
480.313402	20623.716761	30.556237
481.089932	20639.611496	30.561255
481.632878	20674.107143	30.566272
481.892186	20704.774338	30.571290
482.566974	20717.616868	30.576308
482.845091	20738.212155	30.581325
483.067899	20759.087575	30.586343
483.327183	20788.567384	30.591360
484.268023	20815.936050	30.596378
484.709298	20849.731257	30.601396
484.672880	20872.774393	30.606413
485.434892	20902.108574	30.611431
485.853908	20942.611600	30.616448
486.215530	20968.128436	30.621466
486.839292	21003.041917	30.626484
487.333786	21028.689677	30.631501
487.770062	21062.705463	30.636519
487.801984	21101.351382	30.641536
488.539109	21136.484145	30.646554
489.023778	21170.887006	30.651572
489.497869	21201.665076	30.656589
490.287263	21228.864074	30.661607
490.878252	21266.786201	30.666624
491.516408	21295.896325	30.671642
492.224267	21315.215057	30.676660
492.493913	21342.538000	30.681677
493.057242	21370.793898	30.686695
493.733053	21394.460292	30.691712
494.510158	21425.578000	30.696730
494.701712	21449.616156	30.701748
494.993260	21490.442923	30.706765
496.035237	21504.747170	30.711783
495.883428	21535.555508	30.716800
496.470610	21554.719714	30.721818
496.762123	21589.462192	30.726836
497.491451	21624.205096	30.731853
497.908875	21654.901728	30.736871
498.234071	21688.981459	30.741888
498.929716	21721.950084	30.746906
499.558584	21756.595090	30.751924
499.644923	21798.791035	30.756941
500.327216	21822.517686	30.761959
500.715808	21855.145664	30.766976
501.119344	21887.244451	30.771994
501.812765	21921.150258	30.777012
501.934357	21963.987617	30.782029
502.567580	21988.372863	30.787047
503.107615	22027.423287	30.792064
503.396585	22056.217141	30.797082
504.282587	22109.162058	30.802100
504.270863	22146.381361	30.807117
505.095093	22168.851801	30.812135
505.855756	22217.618498	30.817152
506.211051	22257.725133	30.822170
506.719609	22283.064762	30.827188
507.513950	22317.676771	30.832205
508.063956	22351.480338	30.837223
508.450320	22382.607058	30.842240
509.011861	22412.453674	30.847258
509.671508	22441.085225	30.852276
510.202956	22462.478839	30.857293
511.033888	22484.681674	30.862311
511.072805	22501.687382	30.867328
511.343503	22537.308704	30.872346
512.244449	22551.727744	30.877364
512.574846	22587.815377	30.882381
512.996284	22612.507048	30.887399
513.110120	22646.230296	30.892416
513.573934	22673.063876	30.897434
514.274770	22713.040231	30.902452
514.688856	22742.737690	30.907469
515.123394	22773.394398	30.912487
515.876967	22821.938843	30.917504
516.076593	22842.400535	30.922522
516.372709	22884.985763	30.927540
516.888049	22930.829187	30.932557
517.418380	22960.106857	30.937575
518.154070	23008.738999	30.942592
518.849135	23045.213017	30.947610
519.596251	23076.545920	30.952628
520.005517	23116.031009	30.957645
520.394977	23157.268660	30.962663
521.074569	23186.489895	30.967680
521.279256	23220.182567	30.972698
521.867054	23266.854245	30.977716
522.579122	23294.798489	30.982733
523.516803	23329.859320	30.987751
523.843126	23368.480831	30.992768
524.185226	23400.400303	30.997786
525.193361	23435.627365	31.002804
525.326493	23472.080033	31.007821
525.962945	23496.668740	31.012839
526.352861	23527.415934	31.017856
527.041602	23567.397168	31.022874
527.534292	23599.708144	31.027892
528.175650	23636.538647	31.032909
528.970600	23659.376629	31.037927
529.435501	23701.855255	31.042944
529.599469	23729.685935	31.047962
530.321033	23758.054819	31.052980
530.575323	23802.630122	31.057997
531.490330	23831.586635	31.063015
531.862579	23870.695915	31.068032
532.329648	23901.306308	31.073050
532.860752	23933.198325	31.078068
532.979778	23972.605755	31.083085
533.964760	24011.073509	31.088103
534.346870	24041.397605	31.093120
534.790862	24081.182821	31.098138
535.562662	24114.582270	31.103156
535.855481	24148.722089	31.108173
536.277862	24196.683130	31.113191
536.729479	24223.696938	31.118208
537.116454	24273.697628	31.123226
537.839672	24298.397429	31.128244
538.146331	24327.550996	31.133261
538.718397	24362.545539	31.138279
539.264772	24406.977555	31.143296
539.496248	24441.912307	31.148314
540.343127	24480.799406	31.153332
540.656720	24526.489749	31.158349
541.440579	24556.421584	31.163367
542.311637	24599.246732	31.168384
542.764661	24627.848995	31.173402
543.258978	24657.789331	31.178420
543.710984	24705.143812	31.183437
544.238632	24730.058970	31.188455
544.795204	24768.910306	31.193472
545.294741	24813.073646	31.198490
545.687532	24839.558294	31.203508
546.465898	24884.005106	31.208525
547.133807	24926.227813	31.213543
547.660918	24967.953955	31.218560
548.440375	24999.704580	31.223578
549.001101	25034.748886	31.228596
549.176469	25080.988241	31.233613
549.771585	25103.257536	31.238631
550.448276	25149.406214	31.243648
550.807041	25197.976710	31.248666
551.948726	25210.609536	31.253684
552.276508	25259.427773	31.258701
552.536988	25299.615496	31.263719
553.070624	25332.719871	31.268736
553.615476	25378.328559	31.273754
554.321439	25402.279757	31.278772
554.449821	25453.357267	31.283789
555.198427	25483.987312	31.288807
555.970758	25535.210659	31.293824
556.332953	25573.692382	31.298842
557.131923	25616.518361	31.303860
557.684038	25664.671123	31.308877
558.062545	25696.880086	31.313895
558.939748	25740.405273	31.318912
559.177726	25780.296081	31.323930
560.137384	25810.742680	31.328948
560.448316	25848.255627	31.333965
561.284513	25876.505273	31.338983
562.008132	25916.787789	31.344000
562.392989	25955.374745	31.349018
563.378060	25987.914655	31.354036
563.774351	26034.993636	31.359053
563.936097	26052.746131	31.364071
564.747216	26089.530074	31.369088
565.238151	26134.562623	31.374106
566.100185	26154.440963	31.379124
566.437692	26197.189169	31.384141
566.854372	26234.288354	31.389159
567.893220	26254.229254	31.394176
568.141536	26301.837550	31.399194
568.901566	26326.344002	31.404212
569.315782	26340.147649	31.409229
569.730928	26372.210338	31.414247
570.307857	26395.142136	31.419264
570.809502	26432.585902	31.424282
571.405354	26456.353764	31.429300
571.418421	26489.208637	31.434317
571.786135	26528.002953	31.439335
572.764931	26556.640744	31.444352
572.782626	26616.899229	31.449370
573.498606	26650.420822	31.454388
574.011566	26706.386851	31.459405
574.580828	26748.340968	31.464423
575.227983	26784.135574	31.469440
575.869493	26840.780378	31.474458
576.246202	26881.947770	31.479476
576.815890	26931.877260	31.484493
577.398822	26983.869649	31.489511
578.105910	27018.612172	31.494528
578.299216	27070.932388	31.499546
579.478794	27110.114830	31.504564
580.005395	27156.513006	31.509581
580.866694	27201.014509	31.514599
581.680365	27241.475884	31.519616
581.885784	27291.432992	31.524634
582.903376	27326.560036	31.529652
583.227062	27369.424648	31.534669
583.913902	27400.477090	31.539687
584.580294	27428.097111	31.544704
584.868014	27481.208788	31.549722
585.487256	27521.270886	31.554740
586.109535	27567.799186	31.559757
586.461978	27606.443332	31.564775
587.616663	27641.661896	31.569792
588.073269	27681.071960	31.574810
588.880206	27726.889038	31.579828
589.220085	27752.621150	31.584845
589.693456	27804.747090	31.589863
590.347849	27835.841783	31.594880
590.595175	27886.253378	31.599898
591.537545	27935.883185	31.604916
591.828109	27969.960606	31.609933
592.509097	28021.015783	31.614951
593.166017	28063.057065	31.619968
593.540255	28116.655772	31.624986
594.453429	28150.317698	31.630004
594.959122	28185.465904	31.635021
595.305460	28243.235730	31.640039
596.094881	28280.013974	31.645056
596.420268	28333.879604	31.650074
597.134721	28363.774482	31.655092
597.875760	28425.928888	31.660109
598.310267	28473.063281	31.665127
598.807803	28510.759935	31.670144
599.178941	28570.313903	31.675162
600.129489	28610.111640	31.680180
600.729020	28662.943542	31.685197
601.126890	28693.067511	31.690215
602.067607	28729.340494	31.695232
602.530465	28774.113865	31.700250
602.966914	28812.183383	31.705268
603.929502	28854.683880	31.710285
604.371329	28893.219170	31.715303
605.211920	28928.782101	31.720320
605.221664	28981.437926	31.725338
606.194927	29022.544144	31.730356
606.581066	29063.093150	31.735373
607.123215	29100.867593	31.740391
607.987220	29145.244031	31.745408
608.516050	29192.143305	31.750426
609.574749	29236.627663	31.755444
609.940548	29280.960897	31.760461
610.247671	29321.984857	31.765479
610.912170	29357.605138	31.770496
611.004190	29423.311543	31.775514
612.077284	29471.837911	31.780532
612.302878	29512.216623	31.785549
612.922781	29574.848579	31.790567
613.917234	29623.285492	31.795584
614.826769	29670.064061	31.800602
615.531361	29717.519940	31.805620
615.994625	29770.364544	31.810637
616.477711	29816.540115	31.815655
617.389689	29862.105408	31.820672
617.829972	29894.446877	31.825690
618.599172	29938.717666	31.830708
619.553221	29989.420386	31.835725
619.730020	30036.124433	31.840743
620.430570	30066.383984	31.845760
620.937714	30132.698488	31.850778
621.639477	30170.966908	31.855796
621.873000	30215.345817	31.860813
622.694623	30266.300575	31.865831
623.660518	30313.859995	31.870848
623.837906	30368.287033	31.875866
624.638897	30403.796471	31.880884
625.492324	30454.549760	31.885901
626.059901	30503.110858	31.890919
626.415830	30544.030840	31.895936
627.034195	30598.036982	31.900954
627.637483	30647.839419	31.905972
628.116199	30688.409255	31.910989
628.885459	30751.132270	31.916007
629.625880	30793.613343	31.921024
630.037596	30855.780635	31.926042
630.763970	30902.339758	31.931060
631.684772	30940.843029	31.936077
631.999496	31001.180816	31.941095
632.641911	31053.224076	31.946112
633.368473	31084.764258	31.951130
634.047909	31144.672558	31.956148
634.420730	31184.630079	31.961165
634.954229	31235.699941	31.966183
635.752579	31272.858650	31.971200
636.421619	31320.253938	31.976218
637.303145	31361.762091	31.981236
638.071240	31399.282093	31.986253
638.372851	31450.000265	31.991271
638.913985	31493.216236	31.996288
639.181578	31547.517781	32.001306
639.902294	31602.730818	32.006324
640.853756	31640.386086	32.011341
641.041542	31698.781293	32.016359
642.029304	31742.941799	32.021376
642.523529	31800.684933	32.026394
643.232472	31849.169204	32.031412
644.021504	31899.298920	32.036429
644.324331	31955.577359	32.041447
645.217458	32002.959431	32.046464
646.007314	32059.237903	32.051482
646.690644	32103.515631	32.056500
647.651878	32162.110854	32.061517
648.184814	32206.742219	32.066535
649.139856	32256.288644	32.071552
649.563775	32287.770586	32.076570
650.177148	32337.221928	32.081588
651.001289	32377.269681	32.086605
651.472591	32424.294581	32.091623
652.390640	32473.351066	32.096640
653.117008	32532.420028	32.101658
653.569328	32571.318547	32.106676
654.218306	32629.580577	32.111693
654.881818	32676.895555	32.116711
655.531215	32713.624164	32.121728
656.049737	32767.847228	32.126746
656.696483	32819.671588	32.131764
657.669878	32856.268541	32.136781
657.838130	32912.325795	32.141799
658.635524	32957.307984	32.146816
659.233370	33006.982904	32.151834
659.558011	33053.640478	32.156852
660.184602	33111.430186	32.161869
660.806518	33182.459511	32.166887
661.846661	33232.364166	32.171904
662.277347	33297.942327	32.176922
662.915139	33357.233261	32.181940
663.760182	33401.411500	32.186957
664.099489	33472.608442	32.191975
664.784287	33508.664860	32.196992
665.704423	33569.472088	32.202010
666.023522	33631.934166	32.207028
667.080860	33680.455058	32.212045
667.724577	33738.187487	32.217063
668.629907	33793.168839	32.222080
668.969056	33852.327829	32.227098
669.513091	33903.656502	32.232116
670.590307	33944.246273	32.237133
671.219028	33991.515392	32.242151
671.951939	34034.690165	32.247168
672.180044	34080.054524	32.252186
672.856316	34130.327213	32.257204
673.709240	34178.659857	32.262221
673.945049	34220.966900	32.267239
675.130416	34273.659008	32.272256
675.672646	34319.155283	32.277274
676.097870	34390.626230	32.282292
677.374558	34419.391274	32.287309
677.660581	34486.502578	32.292327
678.319807	34528.202302	32.297344
678.895801	34592.682655	32.302362
679.812591	34634.116217	32.307380
680.855590	34679.935721	32.312397
681.282970	34742.019024	32.317415
681.838486	34787.109341	32.322432
682.561484	34840.479047	32.327450
683.029750	34903.363548	32.332468
683.852729	34947.965600	32.337485
684.495757	35000.725881	32.342503
685.253427	35058.178354	32.347520
685.637329	35124.647666	32.352538
686.643739	35175.539356	32.357556
687.248461	35228.541344	32.362573
687.796428	35292.491317	32.367591
688.493905	35341.523657	32.372608
689.412640	35409.644597	32.377626
690.081981	35465.643308	32.382644
690.822484	35512.249470	32.387661
691.204301	35581.906926	32.392679
692.362999	35627.275528	32.397696
692.811462	35691.927056	32.402714
693.576048	35743.901027	32.407732
694.316438	35795.631508	32.412749
695.035267	35852.969944	32.417767
695.710243	35918.932596	32.422784
696.406693	35969.589147	32.427802
697.229615	36030.408264	32.432820
697.901240	36084.241014	32.437837
698.461790	36134.123572	32.442855
699.057808	36188.097967	32.447872
699.704773	36252.242379	32.452890
700.481906	36311.108629	32.457908
701.493524	36371.517428	32.462925
701.928738	36439.071604	32.467943
703.013511	36487.091853	32.472960
703.522189	36544.239100	32.477978
704.051387	36589.986443	32.482996
705.155040	36637.729801	32.488013
705.934956	36696.122422	32.493031
706.397644	36749.143970	32.498048
707.034807	36796.206879	32.503066
707.386207	36855.432912	32.508084
708.383213	36896.231866	32.513101
709.231028	36950.217506	32.518119
709.629450	36992.349606	32.523136
710.139471	37046.274245	32.528154
710.880537	37103.285500	32.533172
711.539306	37154.563357	32.538189
712.406749	37210.835930	32.543207
713.062051	37256.304876	32.548224
713.819925	37317.408628	32.553242
713.928735	37376.299886	32.558260
715.278642	37422.685077	32.563277
715.603075	37492.044288	32.568295
716.283952	37550.471419	32.573312
717.340786	37609.020214	32.578330
717.892181	37679.063009	32.583348
718.459099	37731.743124	32.588365
719.572524	37789.485753	32.593383
720.291690	37834.233449	32.598400
720.966017	37905.086937	32.603418
721.641135	37963.672511	32.608436
722.107817	38016.888201	32.613453
722.930900	38078.955572	32.618471
723.551354	38139.160252	32.623488
724.644816	38203.837028	32.628506
724.972407	38275.836771	32.633524
725.927641	38332.146424	32.638541
726.644630	38402.402369	32.643559
727.182551	38462.159364	32.648576
728.206676	38515.029299	32.653594
728.849664	38594.051792	32.658612
729.330018	38654.901847	32.663629
729.946916	38723.007048	32.668647
730.796516	38791.744020	32.673664
731.921148	38857.288706	32.678682
732.541442	38932.576332	32.683700
733.185206	38987.075600	32.688717
733.893496	39045.963967	32.693735
734.465255	39113.576513	32.698752
735.400209	39174.879558	32.703770
736.201539	39236.814316	32.708788
737.170295	39305.997985	32.713805
737.847033	39364.728497	32.718823
738.595081	39433.570967	32.723840
739.796544	39493.583909	32.728858
740.347214	39553.807890	32.733876
740.784333	39612.542717	32.738893
741.967332	39674.716337	32.743911
742.368798	39725.938904	32.748928
743.036843	39792.961710	32.753946
743.711548	39854.821121	32.758964
744.729030	39904.424504	32.763981
745.387713	39970.881836	32.768999
746.051524	40044.344621	32.774016
746.813619	40104.289329	32.779034
747.472770	40161.439067	32.784052
748.021714	40212.023064	32.789069
748.991493	40256.414019	32.794087
749.761041	40308.787642	32.799104
750.533991	40369.553118	32.804122
750.711777	40433.546857	32.809140
751.918592	40480.705973	32.814157
752.877417	40541.738933	32.819175
752.967166	40601.267312	32.824192
753.825690	40656.728060	32.829210
754.367432	40735.502256	32.834228
755.004244	40792.094704	32.839245
756.204215	40870.611780	32.844263
756.728989	40933.259064	32.849280
757.767238	40997.105325	32.854298
758.167599	41058.700547	32.859316
759.181594	41124.847200	32.864333
759.836836	41181.866941	32.869351
760.393309	41259.289745	32.874368
761.454869	41321.099208	32.879386
762.100401	41402.696952	32.884404
762.848090	41463.695858	32.889421
763.917857	41521.719951	32.894439
764.638741	41596.266890	32.899456
765.376579	41663.598190	32.904474
765.634077	41723.802388	32.909492
766.629000	41804.166817	32.914509
767.321185	41874.212391	32.919527
768.410686	41946.711961	32.924544
769.208830	42017.498233	32.929562
769.942364	42095.085876	32.934580
770.944634	42149.599706	32.939597
771.757233	42234.209077	32.944615
772.248743	42303.042463	32.949632
773.248248	42358.080985	32.954650
773.914300	42434.539100	32.959668
774.645502	42486.157463	32.964685
775.514384	42565.551957	32.969703
776.114836	42641.702861	32.974720
777.160227	42706.055884	32.979738
778.052682	42771.922289	32.984756
778.900556	42851.173198	32.989773
779.505927	42903.891598	32.994791
780.370578	42981.131174	32.999808
781.274004	43029.178355	33.004826
781.798125	43106.526321	33.009844
782.686047	43165.767787	33.014861
783.636705	43234.616981	33.019879
784.035577	43307.222765	33.024896
785.122696	43366.322813	33.029914
785.878182	43439.115273	33.034932
786.864545	43494.534897	33.039949
787.866843	43550.444245	33.044967
788.558750	43630.947464	33.049984
789.322028	43685.810187	33.055002
789.698117	43738.791600	33.060020
790.272964	43798.441523	33.065037
791.228496	43862.456724	33.070055
791.516566	43926.912774	33.075072
792.510824	43985.212725	33.080090
792.813705	44058.016746	33.085108
793.817265	44123.170339	33.090125
794.581213	44188.150966	33.095143
795.229882	44255.421428	33.100160
795.955733	44332.578736	33.105178
796.491710	44408.072627	33.110196
796.977033	44488.899779	33.115213
798.672831	44566.673452	33.120231
799.238184	44646.930246	33.125248
800.140820	44712.392341	33.130266
800.840336	44799.943973	33.135284
801.916310	44876.155218	33.140301
802.542829	44935.179371	33.145319
803.492297	45014.685862	33.150336
804.725520	45085.409162	33.155354
805.015834	45163.759390	33.160372
805.724950	45235.579369	33.165389
807.135303	45312.565835	33.170407
807.605039	45396.144271	33.175424
808.559225	45451.322908	33.180442
809.289133	45532.308420	33.185460
810.035556	45604.288029	33.190477
811.001756	45672.078137	33.195495
811.576264	45747.174209	33.200512
812.626977	45816.238574	33.205530
813.219774	45891.960160	33.210548
813.935979	45981.436349	33.215565
815.455691	46046.808409	33.220583
815.869541	46120.287992	33.225600
816.830036	46205.413781	33.230618
817.612602	46284.277494	33.235636
818.350826	46355.210935	33.240653
819.346006	46428.454163	33.245671
819.688073	46514.657906	33.250688
821.078240	46580.598386	33.255706
822.032930	46652.413507	33.260724
822.608408	46719.963845	33.265741
823.727678	46788.749822	33.270759
824.590416	46864.442120	33.275776
825.416035	46934.805571	33.280794
826.239137	46997.906899	33.285812
826.924635	47069.984272	33.290829
828.014969	47135.870455	33.295847
828.538068	47216.319313	33.300864
829.490849	47281.262494	33.305882
829.918128	47355.410833	33.310900
830.752555	47432.189120	33.315917
831.979783	47489.009242	33.320935
832.428375	47576.450659	33.325952
833.391781	47640.121970	33.330970
834.281202	47722.294326	33.335988
834.883748	47778.482818	33.341005
835.876131	47850.009729	33.346023
836.165825	47917.108486	33.351040
837.025670	47982.539170	33.356058
837.882265	48052.902171	33.361076
838.764603	48124.917836	33.366093
839.692660	48196.648860	33.371111
840.396114	48279.822065	33.376128
840.910838	48348.410624	33.381146
842.168455	48419.695701	33.386164
842.962755	48508.131107	33.391181
843.936722	48581.793726	33.396199
844.663200	48653.523983	33.401216
845.537693	48735.037670	33.406234
846.599211	48816.503036	33.411252
846.767964	48884.580779	33.416269
847.994275	48961.508458	33.421287
848.724311	49052.522113	33.426304
849.534463	49129.324277	33.431322
850.506980	49222.508981	33.436340
851.395154	49307.995773	33.441357
852.130738	49382.012051	33.446375
852.641289	49466.856048	33.451392
853.836483	49549.136548	33.456410
854.724160	49636.644495	33.461428
855.441173	49721.583070	33.466445
856.880927	49807.858559	33.471463
857.561983	49890.629527	33.476480
858.388339	49961.449863	33.481498
859.242612	50056.503748	33.486516
860.376202	50136.130342	33.491533
860.957194	50210.392409	33.496551
861.988151	50289.089350	33.501568
862.816356	50383.025741	33.506586
863.810297	50455.001568	33.511604
864.439913	50535.694706	33.516621
865.881545	50615.586831	33.521639
866.728920	50686.678095	33.526656
867.450846	50764.283970	33.531674
868.417941	50841.264210	33.536692
869.107672	50927.008111	33.541709
870.417752	50999.323978	33.546727
870.778563	51084.474058	33.551744
871.706120	51169.654269	33.556762
872.688106	51242.603991	33.561780
873.348475	51323.592437	33.566797
874.460471	51399.172954	33.571815
875.087838	51484.591785	33.576832
876.051501	51564.400125	33.581850
876.691612	51647.772741	33.586868
877.381906	51736.433257	33.591885
878.792640	51806.694549	33.596903
879.949709	51896.610191	33.601920
880.544748	51970.681676	33.606938
881.903122	52036.543439	33.611956
882.337129	52106.955030	33.616973
882.994225	52162.179845	33.621991
883.537723	52245.365479	33.627008
884.366695	52311.258848	33.632026
885.078489	52399.448983	33.637044
885.898784	52468.648596	33.642061
886.922857	52544.541442	33.647079
887.569792	52642.308871	33.652096
888.796883	52717.441105	33.657114
889.624582	52802.569221	33.662132
890.183813	52889.072311	33.667149
890.988003	52975.331692	33.672167
892.387385	53065.492359	33.677184
893.194834	53150.533816	33.682202
894.258119	53237.346565	33.687220
895.290134	53325.960540	33.692237
896.203120	53396.534505	33.697255
896.793406	53489.022709	33.702272
897.599812	53564.597846	33.707290
898.749457	53659.873176	33.712308
899.251813	53747.588776	33.717325
900.451679	53834.572034	33.722343
901.300285	53931.275960	33.727360
902.311696	54014.228012	33.732378
903.329161	54095.415137	33.737396
904.125315	54193.984688	33.742413
905.045095	54275.317571	33.747431
905.768465	54364.642255	33.752448
907.079014	54454.091730	33.757466
908.179276	54526.966510	33.762484
908.901776	54629.962695	33.767501
909.763657	54714.040153	33.772519
910.748059	54793.654330	33.777536
911.743102	54874.412932	33.782554
912.901758	54964.864420	33.787572
913.486269	55050.209096	33.792589
914.631507	55136.367688	33.797607
915.550978	55220.753969	33.802624
916.297561	55300.887990	33.807642
917.400888	55391.429314	33.812660
918.357498	55476.271715	33.817677
918.979558	55555.296645	33.822695
920.004174	55648.045540	33.827712
920.940805	55738.539356	33.832730
922.022586	55818.650725	33.837748
922.853910	55912.192447	33.842765
923.750828	55984.010094	33.847783
924.678043	56078.954716	33.852800
925.665402	56159.202554	33.857818
926.581253	56240.573254	33.862836
927.124575	56330.498103	33.867853
928.629910	56413.590844	33.872871
929.491024	56511.370275	33.877888
930.142750	56581.281616	33.882906
931.182764	56664.402186	33.887924
931.860249	56748.919262	33.892941
932.876589	56815.544167	33.897959
933.621456	56900.906693	33.902976
934.283124	56987.839132	33.907994
935.721093	57060.345161	33.913012
936.373533	57144.018871	33.918029
937.408556	57222.454950	33.923047
938.272580	57296.814726	33.928064
939.206150	57387.231942	33.933082
940.592946	57468.943548	33.938100
941.050699	57550.553947	33.943117
942.028584	57629.947911	33.948135
942.643372	57714.634088	33.953152
943.597492	57810.331567	33.958170
945.180112	57899.906163	33.963188
945.735444	57990.257088	33.968205
946.917985	58073.980115	33.973223
947.537096	58169.413909	33.978240
948.589113	58269.091739	33.983258
949.548764	58352.782040	33.988276
950.199024	58457.134004	33.993293
951.353492	58541.542373	33.998311
952.303274	58629.124942	34.003328
952.853236	58743.691694	34.008346
954.525286	58815.065586	34.013364
955.112610	58922.353626	34.018381
955.726506	59009.729397	34.023399
956.766547	59106.701699	34.028416
957.936490	59203.511769	34.033434
959.235131	59300.753340	34.038452
960.033527	59406.359408	34.043469
961.111989	59507.438319	34.048487
962.193791	59595.455925	34.053504
962.863609	59697.405970	34.058522
963.788671	59781.894375	34.063540
965.006496	59883.316238	34.068557
965.669350	59981.047708	34.073575
966.852522	60088.768627	34.078592
967.854517	60182.500598	34.083610
969.334058	60279.535386	34.088628
969.871179	60374.229486	34.093645
970.835458	60465.960822	34.098663
971.995026	60550.952154	34.103680
972.810329	60649.569033	34.108698
973.945705	60755.214381	34.113716
974.690439	60848.567536	34.118733
975.862316	60940.242914	34.123751
976.764628	61045.788057	34.128768
977.537201	61130.897272	34.133786
978.637708	61230.254886	34.138804
979.567581	61340.312488	34.143821
980.345070	61434.648490	34.148839
981.760534	61534.049174	34.153856
982.720967	61629.285362	34.158874
983.719905	61705.036961	34.163892
984.715881	61808.718013	34.168909
985.657078	61872.095492	34.173927
986.577329	61955.505122	34.178944
987.500787	62051.946063	34.183962
988.478931	62121.033778	34.188980
989.214119	62230.840228	34.193997
990.257635	62310.654218	34.199015
991.279501	62399.853420	34.204032
992.074437	62491.918430	34.209050
993.114352	62588.940397	34.214068
994.104269	62690.821069	34.219085
994.900477	62793.936205	34.224103
995.929966	62878.428278	34.229120
996.475223	62992.431286	34.234138
997.593987	63083.503493	34.239156
998.371507	63206.953665	34.244173
999.005433	63311.805812	34.249191
1000.412359	63413.371413	34.254208
1001.432014	63535.651545	34.259226
1002.450290	63634.750718	34.264244
1003.437141	63738.311193	34.269261
1005.082213	63854.677055	34.274279
1006.143094	63949.087914	34.279296
1006.833105	64075.712432	34.284314
1008.077261	64165.029863	34.289332
1008.989488	64277.507447	34.294349
1009.879312	64386.938633	34.299367
1011.050089	64486.962237	34.304384
1012.097141	64592.538922	34.309402
1013.502381	64695.036958	34.314420
1014.592460	64805.758759	34.319437
1015.654526	64896.033906	34.324455
1016.707776	64999.063285	34.329472
1017.473347	65100.724147	34.334490
1018.878183	65199.612077	34.339508
1019.801002	65305.417751	34.344525
1020.720769	65404.140726	34.349543
1021.952279	65498.648978	34.354560
1022.817038	65605.498274	34.359578
1024.006709	65706.687487	34.364596
1025.090172	65805.373860	34.369613
1025.880142	65904.072689	34.374631
1026.946704	66004.954603	34.379648
1027.849069	66107.306504	34.384666
1028.943963	66216.481834	34.389684
1029.923469	66317.931946	34.394701
1030.740124	66432.992496	34.399719
1032.129737	66523.103200	34.404736
1033.120901	66621.116773	34.409754
1034.500377	66710.588821	34.414772
1035.945639	66799.716032	34.419789
1037.047627	66904.421855	34.424807
1038.386423	66992.063489	34.429824
1039.098437	67083.794337	34.434842
1040.201717	67153.275233	34.439860
1041.416785	67242.766435	34.444877
1041.667572	67312.879391	34.449895
1042.744183	67385.176412	34.454912
1043.442082	67479.826676	34.459930
1044.323672	67576.216957	34.464948
1045.135682	67669.472882	34.469965
1046.212822	67760.754050	34.474983
1047.229454	67870.320755	34.480000
1047.510291	67972.032844	34.485018
1049.040624	68071.910557	34.490036
1049.742070	68171.731117	34.495053
1050.813710	68273.874917	34.500071
1052.130394	68395.248070	34.505088
1052.986431	68513.795591	34.510106
1054.067979	68630.583317	34.515124
1055.027234	68729.715047	34.520141
1055.710331	68847.521386	34.525159
1057.225920	68965.575069	34.530176
1058.085713	69079.722147	34.535194
1059.108198	69197.849356	34.540212
1060.514778	69315.177027	34.545229
1061.367794	69437.161114	34.550247
1062.664500	69553.812756	34.555264
1063.864926	69668.913615	34.560282
1064.832930	69786.989880	34.565300
1066.424433	69898.163416	34.570317
1067.316228	70004.028178	34.575335
1068.904071	70102.902646	34.580352
1069.979455	70211.354925	34.585370
1071.305737	70319.736309	34.590388
1072.203375	70415.569491	34.595405
1073.185957	70524.000355	34.600423
1074.422258	70627.476032	34.605440
1075.287318	70743.704303	34.610458
1075.895917	70853.017817	34.615476
1077.391034	70958.046235	34.620493
1078.292876	71071.642250	34.625511
1079.752581	71157.558577	34.630528
1080.507525	71295.687576	34.635546
1081.361713	71406.860579	34.640564
1082.668132	71514.057561	34.645581
1083.377304	71631.478440	34.650599
1084.492900	71751.394325	34.655616
1085.461189	71864.358820	34.660634
1086.562675	71987.172222	34.665652
1087.704368	72092.275540	34.670669
1088.539303	72220.358188	34.675687
1090.075110	72336.166921	34.680704
1090.932659	72451.610312	34.685722
1092.189827	72578.048465	34.690740
1093.535644	72692.373023	34.695757
1094.389286	72814.390591	34.700775
1095.600796	72917.496787	34.705792
1096.605034	73040.926155	34.710810
1097.650305	73136.755394	34.715828
1098.825551	73249.189364	34.720845
1099.971535	73335.007092	34.725863
1101.030244	73446.929928	34.730880
1101.984774	73552.557314	34.735898
1102.877708	73658.334075	34.740916
1104.066163	73754.535297	34.745933
1105.147923	73879.107599	34.750951
1106.355254	73973.278453	34.755968
1107.511916	74095.483170	34.760986
1108.462259	74203.212623	34.766004
1109.560492	74318.931892	34.771021
1110.561173	74430.648305	34.776039
1111.787614	74551.492395	34.781056
1112.847964	74662.322233	34.786074
1113.801407	74784.550842	34.791092
1115.414111	74891.723668	34.796109
1116.472123	75012.932257	34.801127
1117.476394	75126.086489	34.806144
1118.731713	75250.191043	34.811162
1119.666706	75361.562881	34.816180
1121.062404	75476.072410	34.821197
1121.940685	75603.651679	34.826215
1122.967131	75708.583849	34.831232
1124.439631	75842.579367	34.836250
1125.298413	75960.235769	34.841268
1126.988769	76064.792464	34.846285
1127.511733	76189.461663	34.851303
1128.930871	76302.543892	34.856320
1130.041575	76423.727318	34.861338
1131.085068	76554.168185	34.866356
1132.321956	76672.463796	34.871373
1133.318370	76788.466267	34.876391
1134.709606	76915.529852	34.881408
1135.767857	77038.488587	34.886426
1136.660937	77158.010922	34.891444
1138.375667	77277.725622	34.896461
1139.163470	77403.693723	34.901479
1140.194765	77508.293175	34.906496
1141.586300	77634.406865	34.911514
1142.628042	77760.248309	34.916532
1143.703101	77883.158924	34.921549
1144.555226	78010.498383	34.926567
1146.041941	78133.231277	34.931584
1147.560203	78262.520509	34.936602
1148.438784	78382.539017	34.941620
1150.044164	78505.817806	34.946637
1151.091601	78628.699384	34.951655
1152.152265	78750.075296	34.956672
1153.398064	78864.457157	34.961690
1154.278253	78970.990651	34.966708
1155.754026	79095.665194	34.971725
1156.601324	79228.600507	34.976743
1157.904774	79325.467339	34.981760
1158.858824	79451.649184	34.986778
1159.780568	79571.225339	34.991796
1160.985482	79663.703810	34.996813
1162.242485	79777.918324	35.001831
1163.257813	79882.930688	35.006848
1164.395954	80006.861698	35.011866
1165.633730	80112.598379	35.016884
1166.697159	80229.361943	35.021901
1167.662726	80355.490612	35.026919
1169.234843	80463.483125	35.031936
1170.484896	80571.685446	35.036954
1171.024595	80702.801811	35.041972
1172.402680	80819.575572	35.046989
1173.122785	80937.320633	35.052007
1174.346666	81063.627472	35.057024
1175.672040	81191.164247	35.062042
1176.843410	81314.946113	35.067060
1177.857465	81449.860461	35.072077
1179.096319	81581.958498	35.077095
1180.608515	81721.681891	35.082112
1181.912411	81835.552645	35.087130
1182.575297	81961.657045	35.092148
1184.231254	82102.232515	35.097165
1185.048451	82232.302957	35.102183
1186.271890	82361.317108	35.107200
1187.459668	82508.563294	35.112218
1188.616656	82636.401227	35.117236
1189.989384	82775.180315	35.122253
1191.036379	82909.144285	35.127271
1192.122549	83041.819539	35.132288
1193.470361	83175.181055	35.137306
1194.583873	83315.250366	35.142324
1196.161508	83437.639985	35.147341
1197.599176	83583.147058	35.152359
1199.027491	83711.353030	35.157376
1199.915691	83847.023603	35.162394
1201.506274	83968.428009	35.167412
1203.032069	84103.410896	35.172429
1204.143263	84209.454066	35.177447
1205.608946	84329.951050	35.182464
1207.018817	84451.039252	35.187482
1208.359905	84577.544705	35.192500
1209.591506	84689.609005	35.197517
1210.884651	84810.357455	35.202535
1211.773062	84914.960149	35.207552
1213.202839	85041.820988	35.212570
1213.702240	85160.807217	35.217588
1215.170829	85279.545178	35.222605
1215.981311	85408.384484	35.227623
1216.828443	85542.852226	35.232640
1218.362658	85667.841354	35.237658
1219.614306	85802.189520	35.242676
1221.094165	85928.668347	35.247693
1222.020546	86048.129098	35.252711
1223.553001	86181.442338	35.257728
1224.296516	86315.469877	35.262746
1225.620651	86432.125416	35.267764
1226.972354	86539.153687	35.272781
1227.928282	86663.336434	35.277799
1228.824919	86774.200411	35.282816
1230.272321	86898.135663	35.287834
1231.352961	87024.286120	35.292852
1232.769179	87147.329899	35.297869
1233.356388	87281.053225	35.302887
1234.752206	87404.152310	35.307904
1236.040335	87540.940067	35.312922
1237.086233	87667.915539	35.317940
1238.702385	87808.762986	35.322957
1240.154633	87936.035871	35.327975
1241.031461	88062.844536	35.332992
1242.419313	88204.325274	35.338010
1243.311799	88333.384187	35.343028
1244.886036	88467.432238	35.348045
1246.264422	88604.787861	35.353063
1247.369833	88740.581565	35.358080
1248.842954	88887.048872	35.363098
1249.671806	89016.830240	35.368116
1251.311932	89151.264136	35.373133
1252.514072	89303.683698	35.378151
1253.335157	89442.802723	35.383168
1255.165088	89578.891234	35.388186
1256.169684	89720.506080	35.393204
1257.620159	89848.309090	35.398221
1259.084014	89997.884109	35.403239
1260.320356	90133.204086	35.408256
1261.653853	90273.960781	35.413274
1262.591476	90406.528399	35.418292
1263.971190	90548.974379	35.423309
1265.708301	90691.851434	35.428327
1266.542842	90841.001065	35.433344
1268.524941	90964.343449	35.438362
1269.245816	91108.396666	35.443380
1270.267116	91245.895346	35.448397
1271.602138	91384.508698	35.453415
1272.875158	91535.515965	35.458432
1274.377256	91662.651026	35.463450
1275.132684	91814.969442	35.468468
1276.886857	91955.100894	35.473485
1278.453562	92103.073883	35.478503
1279.609870	92253.048440	35.483520
1281.142546	92371.676149	35.488538
1282.277105	92506.438802	35.493556
1283.874518	92647.541969	35.498573
1285.032954	92793.136834	35.503591
1286.403006	92923.418291	35.508608
1287.773980	93056.654072	35.513626
1288.818724	93205.843267	35.518644
1290.455765	93327.824373	35.523661
1291.646158	93461.559345	35.528679
1292.779374	93606.543732	35.533696
1294.267757	93730.106637	35.538714
1295.518572	93853.935699	35.543732
1296.619000	93967.068311	35.548749
1297.712607	94081.897719	35.553767
1298.798188	94210.758218	35.558784
1300.254149	94343.381014	35.563802
1301.226238	94471.166801	35.568820
1302.609540	94587.831370	35.573837
1304.083752	94730.574017	35.578855
1304.901586	94859.101310	35.583872
1306.682296	94988.102500	35.588890
1307.569068	95128.410914	35.593908
1308.504394	95267.485350	35.598925
1309.907897	95401.881261	35.603943
1311.459519	95541.827240	35.608960
1312.696126	95697.960742	35.613978
1313.779314	95846.105140	35.618996
1315.165442	95990.229841	35.624013
1316.656047	96139.892835	35.629031
1317.534949	96283.587660	35.634048
1319.143508	96434.467388	35.639066
1320.743286	96584.463907	35.644084
1321.848319	96740.423136	35.649101
1323.406288	96889.530056	35.654119
1324.515389	97039.980829	35.659136
1326.008860	97184.241606	35.664154
1327.653444	97344.382972	35.669172
1328.945915	97481.662006	35.674189
1330.416654	97624.588074	35.679207
1331.510282	97777.564008	35.684224
1333.317890	97925.746090	35.689242
1334.198973	98068.180340	35.694260
1335.716941	98211.361974	35.699277
1337.249943	98362.089436	35.704295
1338.811104	98515.932326	35.709312
1340.364948	98653.069349	35.714330
1340.975748	98801.985112	35.719348
1342.480833	98938.846913	35.724365
1344.259012	99089.818586	35.729383
1345.347493	99238.420860	35.734400
1346.873899	99382.013407	35.739418
1348.376426	99537.700893	35.744436
1349.530276	99675.116406	35.749453
1351.125931	99827.020345	35.754471
1352.370818	99969.376989	35.759488
1354.270551	100109.529931	35.764506
1355.201043	100244.124629	35.769524
1356.326278	100397.170016	35.774541
1357.509485	100520.521234	35.779559
1358.656478	100687.629860	35.784576
1360.496476	100832.484990	35.789594
1362.098067	100984.269084	35.794612
1363.116642	101128.345527	35.799629
1364.590257	101270.015833	35.804647
1365.756853	101418.657730	35.809664
1367.435479	101557.101987	35.814682
1368.843044	101685.137538	35.819700
1369.702637	101820.961189	35.824717
1371.330571	101948.475968	35.829735
1372.309139	102089.590901	35.834752
1373.714144	102233.340714	35.839770
1374.968580	102367.769725	35.844788
1376.120942	102495.457998	35.849805
1377.324472	102654.485304	35.854823
1378.579586	102800.312550	35.859840
1380.240861	102943.665344	35.864858
1381.320598	103097.975980	35.869876
1382.744140	103247.196166	35.874893
1384.129973	103401.624675	35.879911
1385.374547	103557.962321	35.884928
1386.506643	103717.128426	35.889946
1388.247775	103879.432345	35.894964
1389.523521	104033.755951	35.899981
1390.874127	104190.340396	35.904999
1392.308620	104370.148854	35.910016
1393.881580	104518.321908	35.915034
1395.018803	104686.542809	35.920052
1396.536309	104851.369562	35.925069
1398.516913	105011.055026	35.930087
1399.275911	105179.624307	35.935104
1400.559350	105345.358660	35.940122
1402.534504	105500.409696	35.945140
1404.027072	105668.524145	35.950157
1405.306154	105837.844458	35.955175
1406.848035	105993.771274	35.960192
1408.526805	106158.214433	35.965210
1409.843085	106320.735516	35.970228
1411.339403	106480.830580	35.975245
1413.189510	106622.080960	35.980263
1414.367600	106791.145635	35.985280
1415.947396	106938.054323	35.990298
1417.693874	107099.702272	35.995316
1419.089871	107244.907989	36.000333
1420.530129	107409.068565	36.005351
1421.934870	107557.160706	36.010368
1423.254435	107713.691004	36.015386
1424.647598	107871.330841	36.020404
1426.239714	108023.902258	36.025421
1427.937576	108176.527456	36.030439
1429.298785	108322.030010	36.035456
1430.796824	108478.024263	36.040474
1432.007008	108623.476683	36.045492
1433.634630	108774.369993	36.050509
1435.208009	108932.614709	36.055527
1436.617751	109071.531717	36.060544
1437.952458	109221.449026	36.065562
1439.661231	109388.105767	36.070580
1440.405530	109542.239246	36.075597
1442.141921	109676.386125	36.080615
1443.313990	109836.447408	36.085632
1444.945525	109979.163657	36.090650
1446.350396	110130.581828	36.095668
1447.527201	110264.966447	36.100685
1448.901334	110410.403510	36.105703
1450.019173	110553.723769	36.110720
1451.442206	110699.369985	36.115738
1452.964194	110838.057694	36.120756
1453.913146	110995.984614	36.125773
1455.787071	111150.999472	36.130791
1456.754575	111306.842954	36.135808
1458.342596	111466.874123	36.140826
1459.728728	111619.070379	36.145844
1461.254725	111795.159768	36.150861
1462.921161	111936.723498	36.155879
1464.011112	112100.218115	36.160896
1465.755384	112270.579218	36.165914
1467.390598	112431.691585	36.170932
1468.396564	112616.668270	36.175949
1470.145872	112762.167230	36.180967
1471.372562	112930.247628	36.185984
1472.733650	113110.094738	36.191002
1474.122901	113270.194479	36.196020
1475.381645	113452.902628	36.201037
1477.224033	113627.726678	36.206055
1478.994235	113798.081481	36.211072
1480.582771	113973.245817	36.216090
1482.417248	114145.320996	36.221108
1483.434343	114327.250968	36.226125
1485.462832	114472.829512	36.231143
1486.888589	114653.354833	36.236160
1488.626257	114815.029757	36.241178
1490.347063	114983.102434	36.246196
1491.645289	115149.578382	36.251213
1493.236095	115310.412510	36.256231
1494.693773	115482.949234	36.261248
1496.134311	115654.863102	36.266266
1497.722062	115805.558782	36.271284
1499.430526	115992.525325	36.276301
1501.020935	116141.114366	36.281319
1502.396243	116309.212779	36.286336
1503.717418	116473.306990	36.291354
1505.123001	116651.298367	36.296372
1506.955012	116820.239288	36.301389
1508.322069	116972.464793	36.306407
1509.825270	117152.451162	36.311424
1511.460924	117329.271097	36.316442
1513.441969	117476.849856	36.321460
1514.979325	117650.996813	36.326477
1516.506720	117793.831288	36.331495
1518.265437	117966.970188	36.336512
1519.509083	118115.682820	36.341530
1520.941824	118281.904648	36.346548
1522.243084	118446.761822	36.351565
1523.993126	118615.214768	36.356583
1525.114399	118779.779756	36.361600
1526.768988	118942.462862	36.366618
1528.262790	119077.597793	36.371636
1529.442866	119242.909869	36.376653
1530.835112	119382.741716	36.381671
1532.286877	119544.492069	36.386688
1533.451920	119688.679989	36.391706
1535.099200	119850.223897	36.396724
1536.594679	120012.692066	36.401741
1538.212922	120177.427604	36.406759
1539.602593	120349.178415	36.411776
1540.678346	120509.867409	36.416794
1542.379173	120671.547219	36.421812
1543.708511	120859.856837	36.426829
1545.293444	121026.901615	36.431847
1546.864561	121204.385213	36.436864
1548.644820	121379.607821	36.441882
1550.426367	121564.684522	36.446900
1551.803784	121734.160402	36.451917
1553.503610	121908.120175	36.456935
1554.827431	122086.396249	36.461952
1556.440683	122273.923681	36.466970
1558.173169	122451.757357	36.471988
1559.406736	122631.229305	36.477005
1561.462703	122820.045467	36.482023
1563.012939	122997.899103	36.487040
1564.552240	123180.581211	36.492058
1566.231970	123356.149563	36.497076
1567.406163	123547.669419	36.502093
1569.547249	123721.685020	36.507111
1570.965880	123907.089089	36.512128
1572.522322	124098.640847	36.517146
1574.298080	124278.772419	36.522164
1575.427327	124462.947050	36.527181
1577.373497	124645.713900	36.532199
1579.090388	124826.567817	36.537216
1580.647794	125008.765585	36.542234
1582.670922	125190.269958	36.547252
1583.932235	125381.979102	36.552269
1585.771703	125543.881961	36.557287
1587.301311	125734.259003	36.562304
1588.730467	125911.467252	36.567322
1590.336738	126103.443396	36.572340
1591.816653	126291.146884	36.577357
1593.482398	126474.844711	36.582375
1594.784575	126649.417885	36.587392
1596.773130	126843.390618	36.592410
1598.581153	127027.829619	36.597428
1600.026550	127213.467530	36.602445
1601.661994	127397.404416	36.607463
1603.872173	127579.148444	36.612480
1605.268606	127753.574380	36.617498
1606.922551	127925.693009	36.622516
1608.451167	128106.826742	36.627533
1610.407759	128283.269928	36.632551
1612.164863	128455.324826	36.637568
1613.805863	128612.501667	36.642586
1615.437781	128766.741854	36.647604
1616.362485	128927.467311	36.652621
1618.209637	129073.504076	36.657639
1619.466936	129244.604495	36.662656
1620.622627	129407.956401	36.667674
1622.492945	129561.124357	36.672692
1624.080976	129724.409463	36.677709
1625.398804	129891.881073	36.682727
1626.959588	130074.200792	36.687744
1628.685306	130250.173802	36.692762
1630.280238	130431.628964	36.697780
1631.690387	130606.184760	36.702797
1633.063151	130783.496755	36.707815
1634.984327	130967.716105	36.712832
1636.470123	131158.492428	36.717850
1637.959748	131331.722537	36.722868
1639.309777	131528.718200	36.727885
1641.490581	131726.242110	36.732903
1643.230150	131913.144424	36.737920
1645.033005	132101.494929	36.742938
1646.703150	132293.884056	36.747956
1647.755606	132501.880384	36.752973
1649.727101	132688.915708	36.757991
1651.378342	132887.114665	36.763008
1652.718995	133080.575063	36.768026
1654.753544	133281.896078	36.773044
1656.484662	133484.989855	36.778061
1658.250963	133672.000895	36.783079
1660.015045	133865.513415	36.788096
1661.695177	134062.917739	36.793114
1663.666713	134242.791798	36.798132
1665.064329	134455.524372	36.803149
1666.776451	134643.614705	36.808167
1668.437213	134830.840141	36.813184
1670.456230	135035.014231	36.818202
1672.335041	135223.563382	36.823220
1673.867689	135415.336502	36.828237
1675.728941	135610.112457	36.833255
1677.297764	135800.450550	36.838272
1678.746375	136000.008354	36.843290
1680.756581	136187.415179	36.848308
1682.215437	136378.952972	36.853325
1683.881775	136570.446405	36.858343
1686.136362	136755.321789	36.863360
1687.296384	136952.765109	36.868378
1689.480514	137129.797587	36.873396
1691.177814	137330.326089	36.878413
1692.719493	137523.036725	36.883431
1694.719908	137708.883560	36.888448
1696.077488	137908.430854	36.893466
1698.095900	138090.032079	36.898484
1699.735201	138277.561898	36.903501
1701.241879	138463.948112	36.908519
1703.075157	138647.799839	36.913536
1704.470653	138840.884470	36.918554
1706.394472	139017.830261	36.923572
1707.752712	139194.879592	36.928589
1709.573487	139363.099654	36.933607
1711.215069	139531.906728	36.938624
1712.522522	139705.380753	36.943642
1714.353434	139878.189711	36.948660
1715.946225	140060.871772	36.953677
1717.641655	140248.050287	36.958695
1719.754693	140417.649287	36.963712
1720.545950	140604.466675	36.968730
1722.642496	140783.005029	36.973748
1724.289883	140989.788828	36.978765
1725.933868	141185.637330	36.983783
1727.853781	141375.207875	36.988800
1729.311486	141569.352163	36.993818
1730.982103	141764.021537	36.998836
1732.531280	141955.441592	37.003853
1734.480746	142166.748073	37.008871
1736.482633	142366.273532	37.013888
1738.065057	142578.743799	37.018906
1739.958890	142775.868347	37.023924
1741.402346	142973.838812	37.028941
1743.303791	143187.416024	37.033959
1745.512671	143386.737857	37.038976
1747.058944	143596.483263	37.043994
1748.969555	143793.206122	37.049012
1750.507935	144001.333195	37.054029
1752.715178	144199.608569	37.059047
1754.518395	144411.562173	37.064064
1755.949136	144617.897993	37.069082
1757.773871	144812.828477	37.074100
1759.626199	145014.993298	37.079117
1761.108049	145224.620573	37.084135
1763.298169	145434.859300	37.089152
1764.830961	145651.110536	37.094170
1766.765496	145857.285875	37.099188
1768.618248	146060.255974	37.104205
1770.226831	146275.295322	37.109223
1772.283127	146480.111821	37.114240
1774.107124	146689.555175	37.119258
1776.316595	146891.916291	37.124276
1777.986769	147091.334778	37.129293
1779.152389	147300.899403	37.134311
1781.366043	147502.021521	37.139328
1783.059851	147723.433320	37.144346
1784.846813	147914.167933	37.149364
1786.834861	148125.356770	37.154381
1788.426571	148337.788845	37.159399
1790.487078	148526.138561	37.164416
1791.888463	148740.378248	37.169434
1794.136755	148932.173941	37.174452
1796.115752	149146.755660	37.179469
1797.771599	149354.024866	37.184487
1799.655267	149550.572587	37.189504
1801.592692	149743.271843	37.194522
1803.053572	149933.956189	37.199540
1805.083964	150101.909856	37.204557
1806.665853	150288.013311	37.209575
1808.388104	150462.521188	37.214592
1810.265490	150639.667624	37.219610
1811.653356	150829.443394	37.224628
1813.206598	151026.192004	37.229645
1814.966456	151209.014373	37.234663
1816.629304	151404.201203	37.239680
1818.373013	151617.150547	37.244698
1820.208034	151814.036666	37.249716
1822.340171	152011.941748	37.254733
1823.977821	152228.702596	37.259751
1825.644303	152430.360735	37.264768
1827.241027	152632.867939	37.269786
1829.221910	152837.952472	37.274804
1831.181489	153056.125656	37.279821
1833.325535	153272.889054	37.284839
1834.728765	153473.302158	37.289856
1836.203125	153685.749783	37.294874
1838.283290	153902.616185	37.299892
1840.281409	154121.576331	37.304909
1842.040141	154351.999497	37.309927
1844.096080	154554.204632	37.314944
1846.081708	154786.648750	37.319962
1847.386770	155001.959024	37.324980
1849.954633	155216.943434	37.329997
1851.575760	155436.960987	37.335015
1853.612168	155656.584394	37.340032
1855.557465	155877.745215	37.345050
1857.881926	156082.503501	37.350068
1859.607699	156313.591973	37.355085
1861.471565	156536.608547	37.360103
1863.570786	156733.938228	37.365120
1865.881350	156956.873970	37.370138
1867.606380	157156.978963	37.375156
1869.947780	157370.554794	37.380173
1871.428597	157576.977561	37.385191
1873.464411	157781.855268	37.390208
1875.044338	157999.588139	37.395226
1876.684871	158208.094243	37.400244
1878.854453	158416.542994	37.405261
1880.476960	158631.952599	37.410279
1883.064609	158839.094863	37.415296
1884.584473	159056.755156	37.420314
1886.737112	159261.902062	37.425332
1888.586264	159469.964180	37.430349
1890.607037	159677.569153	37.435367
1892.726129	159882.788440	37.440384
1894.252441	160103.282058	37.445402
1896.124189	160304.599309	37.450420
1898.403779	160503.354814	37.455437
1900.003243	160718.058117	37.460455
1901.880096	160916.740383	37.465472
1903.702253	161120.720537	37.470490
1905.416640	161320.369270	37.475508
1907.238519	161508.702925	37.480525
1908.927675	161690.768631	37.485543
1911.122994	161875.354651	37.490560
1912.755315	162060.398749	37.495578
1914.286611	162266.891874	37.500596
1916.217459	162460.476163	37.505613
1917.917963	162655.962284	37.510631
1919.744668	162855.893465	37.515648
1921.923747	163069.098576	37.520666
1923.520140	163278.985957	37.525684
1925.707411	163482.363634	37.530701
1927.304464	163709.336214	37.535719
1929.635026	163907.493845	37.540736
1931.344519	164125.662382	37.545754
1933.055759	164344.948001	37.550772
1935.075520	164559.531505	37.555789
1936.880937	164780.301329	37.560807
1939.204075	165003.019544	37.565824
1941.001586	165222.195273	37.570842
1943.091260	165449.062446	37.575860
1944.907566	165677.737319	37.580877
1946.716326	165904.220657	37.585895
1949.095213	166125.985601	37.590912
1951.110916	166350.840771	37.595930
1952.996189	166575.832150	37.600948
1955.279191	166784.032567	37.605965
1957.423910	167014.210922	37.610983
1959.662400	167235.928670	37.616000
1961.672749	167457.975656	37.621018
1963.813348	167664.123488	37.626036
1965.799866	167869.573936	37.631053
1967.525214	168088.093095	37.636071
1969.673740	168310.338811	37.641088
1971.642555	168522.251659	37.646106
1973.197395	168747.625590	37.651124
1975.598964	168951.937929	37.656141
1977.814210	169185.758663	37.661159
1980.011799	169393.581175	37.666176
1981.852864	169593.647932	37.671194
1983.780677	169817.028321	37.676212
1986.043226	170025.998230	37.681229
1988.103955	170238.223140	37.686247
1990.257315	170449.330973	37.691264
1992.215048	170662.373685	37.696282
1994.201456	170863.705129	37.701300
1996.434575	171067.218290	37.706317
1998.534756	171270.880462	37.711335
2000.662292	171480.374372	37.716352
2002.323887	171686.860918	37.721370
2004.347042	171888.686552	37.726388
2006.460654	172095.192328	37.731405
2008.145118	172316.862526	37.736423
2010.411924	172513.210821	37.741440
2012.193288	172698.765904	37.746458
2014.000759	172908.191384	37.751476
2016.186841	173087.176537	37.756493
2018.139942	173270.563239	37.761511
2019.997089	173444.629531	37.766528
2021.673557	173636.434209	37.771546
2023.718686	173830.299808	37.776564
2025.769548	174019.877699	37.781581
2027.650907	174228.905170	37.786599
2029.915008	174422.421761	37.791616
2031.758040	174614.407682	37.796634
2033.859343	174811.047317	37.801652
2035.879002	175010.238054	37.806669
2038.112157	175203.002161	37.811687
2040.114968	175409.174839	37.816704
2042.148498	175618.578656	37.821722
2044.121253	175810.714609	37.826740
2046.682004	176017.068268	37.831757
2048.148598	176231.512829	37.836775
2050.185170	176417.856564	37.841792
2052.319835	176625.333872	37.846810
2054.501924	176848.662836	37.851828
2056.554198	177048.048678	37.856845
2058.564030	177255.219124	37.861863
2061.045978	177468.887419	37.866880
2063.010179	177680.025486	37.871898
2064.845547	177882.494595	37.876916
2067.070561	178090.853024	37.881933
2069.120559	178313.893693	37.886951
2071.257480	178516.571788	37.891968
2073.492622	178719.704706	37.896986
2075.620414	178950.006126	37.902004
2077.659457	179156.902295	37.907021
2079.856407	179359.625695	37.912039
2081.957383	179570.409064	37.917056
2084.062455	179782.499638	37.922074
2086.306096	179997.347846	37.927092
2088.513747	180201.494583	37.932109
2090.692706	180409.998694	37.937127
2092.807386	180618.945403	37.942144
2095.272415	180823.193856	37.947162
2097.296365	181032.296544	37.952180
2099.551600	181229.931830	37.957197
2101.672816	181431.065766	37.962215
2103.862393	181638.127756	37.967232
2105.832182	181832.486850	37.972250
2107.359498	182052.394637	37.977268
2109.960198	182234.348029	37.982285
2111.920820	182453.313632	37.987303
2114.192473	182660.050282	37.992320
2116.518472	182864.736474	37.997338
2118.457223	183070.347862	38.002356
2120.514738	183263.367152	38.007373
2122.837440	183467.003543	38.012391
2124.648362	183670.519043	38.017408
2127.011251	183856.919837	38.022426
2128.859163	184048.021771	38.027444
2131.451608	184223.234383	38.032461
2133.265553	184404.940925	38.037479
2135.140572	184581.854845	38.042496
2137.204277	184749.730461	38.047514
2139.099335	184942.402179	38.052532
2141.172351	185127.991444	38.057549
2143.252993	185318.871582	38.062567
2145.146538	185507.130196	38.067584
2147.100287	185695.037442	38.072602
2149.040689	185900.103338	38.077620
2151.561646	186093.416685	38.082637
2153.354449	186311.323969	38.087655
2154.955896	186533.653163	38.092672
2157.516610	186732.850783	38.097690
2159.516211	186958.583102	38.102708
2161.894198	187168.496132	38.107725
2163.913647	187394.747722	38.112743
2166.104509	187613.930485	38.117760
2168.500220	187826.419708	38.122778
2170.665707	188048.083050	38.127796
2173.235386	188260.305569	38.132813
2175.181722	188484.987866	38.137831
2177.509099	188704.826704	38.142848
2179.859357	188921.795010	38.147866
2182.174059	189137.945108	38.152884
2184.587286	189357.329246	38.157901
2186.831999	189582.578615	38.162919
2188.999298	189792.016616	38.167936
2191.619266	190005.761903	38.172954
2193.429131	190225.448815	38.177972
2195.897152	190434.321658	38.182989
2198.129845	190652.572920	38.188007
2200.198464	190868.681122	38.193024
2202.790942	191081.483813	38.198042
2204.833680	191296.468588	38.203060
2206.692791	191512.777895	38.208077
2209.242240	191728.737566	38.213095
2211.695892	191942.416360	38.218112
2214.200475	192157.420560	38.223130
2216.158918	192378.413598	38.228148
2218.071991	192587.282266	38.233165
2220.293830	192803.895148	38.238183
2222.634541	193032.787794	38.243200
2225.121133	193236.783742	38.248218
2227.078721	193459.330109	38.253236
2229.396930	193670.842360	38.258253
2231.612609	193888.996635	38.263271
2233.943831	194103.326138	38.268288
2236.442685	194327.668889	38.273306
2238.557457	194538.290621	38.278324
2241.322041	194756.691629	38.283341
2243.758788	194956.450888	38.288359
2245.525104	195177.893019	38.293376
2247.810814	195370.672096	38.298394
2249.753633	195565.701950	38.303412
2251.667085	195747.372777	38.308429
2253.610767	195943.051226	38.313447
2255.463680	196132.487730	38.318464
2257.671939	196329.572581	38.323482
2259.425768	196540.348729	38.328500
2261.832725	196749.029529	38.333517
2264.123167	196953.135123	38.338535
2266.168260	197166.672599	38.343552
2268.196483	197389.009307	38.348570
2270.364489	197618.775141	38.353588
2272.563635	197840.020530	38.358605
2274.963586	198065.918488	38.363623
2276.856736	198302.584780	38.368640
2279.473453	198533.311570	38.373658
2281.315502	198770.292688	38.378676
2283.306102	199015.755333	38.383693
2286.001600	199266.806333	38.388711
2288.319748	199509.300020	38.393728
2290.771170	199752.319465	38.398746
2293.343402	199991.094157	38.403764
2295.635015	200245.970871	38.408781
2297.968549	200492.198267	38.413799
2299.992701	200741.407916	38.418816
2302.917386	200969.595893	38.423834
2305.074051	201231.771751	38.428852
2307.583444	201472.771546	38.433869
2310.380890	201721.482277	38.438887
2312.300070	201973.087823	38.443904
2314.874733	202200.739852	38.448922
2317.301351	202450.972403	38.453940
2319.344780	202716.917834	38.458957
2321.723151	202948.818274	38.463975
2324.169387	203195.065307	38.468992
2326.583663	203456.169996	38.474010
2328.487937	203703.330267	38.479028
2331.218631	203938.631612	38.484045
2334.038589	204187.032437	38.489063
2336.141164	204455.350439	38.494080
2338.690407	204686.113874	38.499098
2340.945525	204930.875493	38.504116
2343.246588	205183.958122	38.509133
2345.266817	205432.745025	38.514151
2347.686730	205681.558491	38.519168
2350.228774	205929.185801	38.524186
2352.544004	206176.012305	38.529204
2355.231961	206440.083027	38.534221
2357.710232	206673.036351	38.539239
2359.671775	206934.457096	38.544256
2361.922150	207170.774437	38.549274
2364.354279	207428.352520	38.554292
2366.584116	207690.305313	38.559309
2369.028879	207945.700169	38.564327
2371.334522	208203.212782	38.569344
2373.664178	208437.491423	38.574362
2375.819487	208678.019029	38.579380
2378.206950	208897.742132	38.584397
2380.622248	209121.473180	38.589415
2382.704215	209364.249413	38.594432
2384.994459	209589.385739	38.599450
2387.235908	209819.342017	38.604468
2389.571828	210053.917855	38.609485
2392.117949	210305.980447	38.614503
2394.405598	210552.753087	38.619520
2396.676781	210777.795196	38.624538
2398.843094	211043.999911	38.629556
2401.139318	211291.053395	38.634573
2403.934775	211531.541406	38.639591
2406.002768	211804.798116	38.644608
2408.242924	212070.931970	38.649626
2410.549294	212333.412836	38.654644
2412.826001	212597.270594	38.659661
2415.484862	212869.955759	38.664679
2417.574799	213136.435222	38.669696
2420.170304	213409.272350	38.674714
2422.669665	213695.088203	38.679732
2424.836446	213968.744668	38.684749
2427.412128	214253.141618	38.689767
2430.038390	214532.669244	38.694784
2432.882817	214805.891668	38.699802
2435.335749	215095.732850	38.704820
2437.709938	215379.646010	38.709837
2440.437246	215646.669357	38.714855
2442.812949	215942.772906	38.719872
2445.427146	216204.280850	38.724890
2448.037924	216492.871461	38.729908
2450.376719	216774.663079	38.734925
2453.123598	217049.852540	38.739943
2455.342680	217330.484634	38.744960
2458.037204	217599.742649	38.749978
2460.741097	217885.442202	38.754996
2463.227289	218153.770428	38.760013
2465.638438	218434.858968	38.765031
2468.282680	218717.651120	38.770048
2470.829988	218998.986937	38.775066
2473.058754	219274.775070	38.780084
2475.362069	219550.539745	38.785101
2477.940034	219829.918639	38.790119
2480.134665	220109.600598	38.795136
2483.105385	220394.594927	38.800154
2485.422389	220685.445709	38.805172
2487.751902	220960.525908	38.810189
2490.367622	221268.523450	38.815207
2492.542672	221599.408898	38.820224
2495.096629	221880.145240	38.825242
2497.663525	222171.914492	38.830260
2500.024541	222455.743583	38.835277
2502.840845	222750.865709	38.840295
2505.451775	223038.530048	38.845312
2508.029765	223308.195698	38.850330
2510.299143	223578.342906	38.855348
2512.582405	223820.655860	38.860365
2515.164954	224078.019546	38.865383
2516.944396	224344.018741	38.870400
2520.047468	224597.581234	38.875418
2522.130642	224866.975113	38.880436
2524.368001	225141.729308	38.885453
2527.045395	225410.459449	38.890471
2529.267813	225688.646275	38.895488
2531.751816	225964.824431	38.900506
2534.242640	226250.081445	38.905524
2536.785703	226531.128148	38.910541
2539.063218	226822.173116	38.915559
2541.621191	227120.704600	38.920576
2544.043952	227413.925377	38.925594
2546.695252	227704.723711	38.930612
2549.550857	228006.131742	38.935629
2552.334408	228306.993534	38.940647
2554.474851	228615.221695	38.945664
2556.878225	228919.472814	38.950682
2559.492891	229228.745463	38.955700
2561.890946	229541.202731	38.960717
2565.191061	229842.927670	38.965735
2567.357023	230159.004858	38.970752
2570.001096	230471.477213	38.975770
2572.824769	230785.242850	38.980788
2575.075428	231099.252749	38.985805
2577.967087	231408.158891	38.990823
2581.162093	231724.357862	38.995840
2583.691949	232036.828281	39.000858
2586.470735	232346.669753	39.005876
2588.889564	232669.623683	39.010893
2591.829506	232969.511183	39.015911
2593.995783	233289.561097	39.020928
2596.996169	233607.270304	39.025946
2599.793470	233915.717065	39.030964
2602.010728	234223.647150	39.035981
2604.763432	234540.535111	39.040999
2607.272248	234860.637509	39.046016
2609.728777	235168.278643	39.051034
2612.376063	235487.218184	39.056052
2614.840737	235802.022311	39.061069
2618.079422	236120.235183	39.066087
2620.439203	236452.430542	39.071104
2622.824446	236759.224214	39.076122
2626.123750	237067.677289	39.081140
2628.319233	237393.704366	39.086157
2631.299090	237705.664158	39.091175
2633.955928	238015.186931	39.096192
2636.374024	238349.385529	39.101210
2639.110262	238663.012225	39.106228
2641.906699	238974.801536	39.111245
2644.610572	239292.067239	39.116263
2647.087658	239615.872012	39.121280
2649.453631	239912.670303	39.126298
2652.209559	240206.258054	39.131316
2654.546378	240509.285395	39.136333
2656.990733	240791.189394	39.141351
2659.576247	241086.584354	39.146368
2662.041408	241375.826979	39.151386
2664.723794	241667.601282	39.156404
2667.233362	241979.012389	39.161421
2669.855430	242281.160894	39.166439
2672.439843	242584.865517	39.171456
2674.605131	242902.302526	39.176474
2677.338030	243208.499770	39.181492
2680.045849	243542.794367	39.186509
2682.887183	243859.745709	39.191527
2685.250063	244182.234700	39.196544
2687.630487	244515.059681	39.201562
2690.244867	244853.233350	39.206580
2692.763962	245200.948179	39.211597
2695.844612	245532.369382	39.216615
2698.370646	245884.733194	39.221632
2700.679015	246248.410316	39.226650
2703.802467	246583.357994	39.231668
2706.553553	246937.289092	39.236685
2709.439110	247288.710487	39.241703
2712.432286	247647.710592	39.246720
2715.067956	248003.135862	39.251738
2718.013933	248353.889842	39.256756
2720.509806	248713.276132	39.261773
2723.604659	249065.430664	39.266791
2726.565577	249422.585872	39.271808
2729.114500	249776.200170	39.276826
2732.214832	250125.993923	39.281844
2734.698824	250478.197598	39.286861
2737.643249	250843.868117	39.291879
2740.593694	251203.645338	39.296896
2743.238265	251557.731019	39.301914
2745.885001	251922.993835	39.306932
2748.622644	252274.322888	39.311949
2751.640078	252621.721870	39.316967
2754.255961	252992.758023	39.321984
2757.109216	253356.035180	39.327002
2759.918303	253708.219417	39.332020
2762.675814	254075.526666	39.337037
2765.610020	254431.426543	39.342055
2768.689552	254795.966173	39.347072
2771.226806	255157.315494	39.352090
2774.025454	255521.418314	39.357108
2776.734578	255879.388637	39.362125
2779.707428	256236.606556	39.367143
2782.666964	256592.226850	39.372160
2785.075819	256956.673350	39.377178
2788.025361	257309.502158	39.382196
2791.091155	257665.056580	39.387213
2794.278340	258036.189448	39.392231
2796.802617	258381.110909	39.397248
2799.459914	258721.464759	39.402266
2802.585377	259055.165691	39.407284
2805.276882	259375.751853	39.412301
2807.722704	259680.475289	39.417319
2810.142726	260004.356780	39.422336
2812.512042	260334.495767	39.427354
2815.393601	260655.637696	39.432372
2817.775034	261003.201857	39.437389
2820.463890	261349.549246	39.442407
2823.165756	261696.276040	39.447424
2825.578084	262054.150140	39.452442
2828.488240	262401.810092	39.457460
2831.068978	262781.022204	39.462477
2833.853375	263141.226531	39.467495
2836.737015	263514.345653	39.472512
2838.995993	263903.009122	39.477530
2842.061775	264271.705520	39.482548
2845.341584	264663.891630	39.487565
2848.271878	265051.764174	39.492583
2850.862628	265436.439278	39.497600
2853.286981	265823.808430	39.502618
2856.690158	266212.115298	39.507636
2859.084833	266624.613597	39.512653
2862.251848	267007.014223	39.517671
2865.257966	267417.561992	39.522688
2868.071547	267821.002281	39.527706
2871.360220	268221.420888	39.532724
2873.883345	268629.861416	39.537741
2876.915388	269040.330130	39.542759
2879.886999	269447.404647	39.547776
2882.545587	269858.517301	39.552794
2885.623168	270252.848468	39.557812
2888.927632	270670.692824	39.562829
2891.857230	271078.054354	39.567847
2894.942356	271483.816442	39.572864
2897.431863	271910.148123	39.577882
2900.348615	272314.133562	39.582900
2903.649261	272724.587033	39.587917
2906.769637	273129.302597	39.592935
2909.890964	273545.830700	39.597952
2912.852517	273966.829788	39.602970
2916.029636	274359.114370	39.607988
2918.951868	274770.466517	39.613005
2921.843863	275179.562586	39.618023
2924.881826	275579.693566	39.623040
2927.751992	275988.285052	39.628058
2931.025481	276384.034759	39.633076
2934.071345	276789.422968	39.638093
2937.028817	277181.183495	39.643111
2939.856458	277584.548475	39.648128
2942.930219	277985.537307	39.653146
2945.925894	278382.931129	39.658164
2948.706614	278781.349609	39.663181
2951.669361	279196.302161	39.668199
2954.767217	279585.626580	39.673216
2957.160887	279980.651067	39.678234
2960.287336	280350.638706	39.683252
2962.981000	280724.987864	39.688269
2966.018262	281088.257417	39.693287
2968.762588	281461.759896	39.698304
2971.254495	281833.523905	39.703322
2974.030072	282206.792405	39.708340
2976.699370	282592.220271	39.713357
2979.901315	282975.607525	39.718375
2982.786361	283363.566456	39.723392
2985.827501	283759.858056	39.728410
2988.481518	284153.797321	39.733428
2991.549620	284565.783185	39.738445
2994.427558	284963.039551	39.743463
2997.394051	285370.823841	39.748480
3000.194679	285788.388783	39.753498
3002.976817	286203.390511	39.758516
3006.050265	286619.082377	39.763533
3008.902192	287051.244597	39.768551
3011.882125	287469.236574	39.773568
3014.942253	287909.823986	39.778586
3017.944641	288345.974446	39.783604
3020.942597	288790.203136	39.788621
3024.074735	289231.590241	39.793639
3027.377048	289670.714321	39.798656
3030.086155	290125.909971	39.803674
3033.571180	290562.692122	39.808692
3036.653669	291017.166753	39.813709
3039.543909	291464.355075	39.818727
3043.035637	291912.666756	39.823744
3045.864571	292365.299360	39.828762
3049.243979	292806.209662	39.833780
3052.323417	293262.763733	39.838797
3055.567480	293705.471946	39.843815
3059.021673	294151.829382	39.848832
3062.138159	294601.465456	39.853850
3065.151228	295050.710525	39.858868
3067.995891	295495.307285	39.863885
3071.459476	295950.499441	39.868903
3074.341437	296397.679350	39.873920
3077.465777	296853.532783	39.878938
3080.672190	297291.006532	39.883956
3083.834864	297733.490367	39.888973
3087.115520	298192.770495	39.893991
3090.300729	298641.446623	39.899008
3093.256794	299081.622905	39.904026
3096.489127	299519.900041	39.909044
3099.902360	299969.247922	39.914061
3102.686347	300421.158122	39.919079
3105.933291	300862.096609	39.924096
3109.049402	301319.082867	39.929114
3112.202856	301761.583166	39.934132
3115.592874	302202.266696	39.939149
3118.393263	302644.896549	39.944167
3121.862496	303081.094408	39.949184
3124.507220	303526.083197	39.954202
3127.680979	303933.393550	39.959220
3130.880265	304344.127834	39.964237
3133.465880	304748.633238	39.969255
3136.625589	305144.359596	39.974272
3139.578214	305557.567832	39.979290
3142.352388	305972.428691	39.984308
3145.162003	306394.471002	39.989325
3147.754027	306831.075430	39.994343
3151.231612	307260.222999	39.999360
3154.051374	307714.822652	40.004378
3157.179762	308151.261557	40.009396
3160.305284	308597.173619	40.014413
3163.362225	309053.102510	40.019431
3166.653957	309503.760185	40.024448
3169.692946	309977.722345	40.029466
3173.011750	310434.620578	40.034484
3176.036437	310904.161748	40.039501
3179.061755	311380.380972	40.044519
3182.510761	311835.322727	40.049536
3185.982396	312322.566906	40.054554
3189.179687	312787.450326	40.059572
3192.414059	313261.469564	40.064589
3195.448933	313749.513094	40.069607
3198.863619	314222.026451	40.074624
3202.222315	314706.788721	40.079642
3205.466470	315184.048892	40.084660
3209.049608	315666.942483	40.089677
3211.834517	316155.649292	40.094695
3215.453042	316621.566666	40.099712
3218.504230	317125.871911	40.104730
3221.446937	317605.301751	40.109748
3224.950120	318105.314390	40.114765
3228.186555	318595.791702	40.119783
3231.646155	319091.894836	40.124800
3234.930944	319586.499161	40.129818
3237.866353	320083.848233	40.134836
3241.756423	320574.668917	40.139853
3245.012700	321080.266677	40.144871
3248.442983	321560.030857	40.149888
3251.480453	322051.232318	40.154906
3255.126615	322542.842686	40.159924
3258.521638	323031.290053	40.164941
3261.123828	323532.609000	40.169959
3264.509712	324025.115557	40.174976
3267.802788	324536.071409	40.179994
3270.814747	325030.891455	40.185012
3274.493351	325531.901223	40.190029
3277.574905	326049.484057	40.195047
3281.035799	326528.123281	40.200064
3284.392301	327037.732926	40.205082
3287.486385	327544.231823	40.210100
3290.808689	328040.050906	40.215117
3294.202671	328548.476673	40.220135
3297.743797	329055.555301	40.225152
3300.860671	329533.671883	40.230170
3303.988981	330002.108438	40.235188
3307.329290	330472.565461	40.240205
3310.220452	330929.758743	40.245223
3313.361971	331385.436760	40.250240
3316.400855	331856.821418	40.255258
3319.182211	332329.488023	40.260276
3322.710165	332802.998392	40.265293
3325.611990	333291.637354	40.270311
3329.250368	333778.201202	40.275328
3332.099715	334273.164495	40.280346
3335.187436	334772.276341	40.285364
3338.687370	335271.344779	40.290381
3341.872908	335780.641562	40.295399
3345.416736	336289.420805	40.300416
3348.990503	336805.707436	40.305434
3351.703237	337337.640498	40.310452
3355.328477	337847.131342	40.315469
3358.257309	338381.992589	40.320487
3362.161174	338914.613187	40.325504
3365.588532	339453.855555	40.330522
3368.446791	339983.661918	40.335540
3372.274075	340521.689426	40.340557
3375.503899	341076.919743	40.345575
3378.837008	341608.236904	40.350592
3382.327460	342163.060838	40.355610
3385.928378	342720.782069	40.360628
3389.520139	343273.701075	40.365645
3392.819246	343818.181377	40.370663
3396.286136	344377.279490	40.375680
3400.030465	344926.757006	40.380698
3403.366782	345486.855422	40.385716
3407.048745	346030.061564	40.390733
3410.369895	346580.148975	40.395751
3414.135329	347139.097283	40.400768
3417.626850	347689.400977	40.405786
3420.802939	348240.561581	40.410804
3424.677578	348782.086284	40.415821
3427.963275	349345.785128	40.420839
3431.974297	349894.512580	40.425856
3435.701889	350447.721916	40.430874
3438.728911	350984.916446	40.435892
3442.481832	351530.825031	40.440909
3445.737214	352086.529284	40.445927
3449.151812	352627.225434	40.450944
3452.826246	353188.893533	40.455962
3456.361425	353733.722375	40.460980
3460.213588	354268.240203	40.465997
3463.639100	354820.004892	40.471015
3467.193482	355362.579797	40.476032
3470.571153	355901.064774	40.481050
3473.858269	356448.747045	40.486068
3477.579721	356986.125422	40.491085
3480.888679	357535.543818	40.496103
3484.257474	358092.434461	40.501120
3487.966796	358607.458056	40.506125
3491.146088	359106.603234	40.511130
3494.302579	359529.560321	40.516135
3497.057283	359941.609921	40.521140
3499.511799	360274.439077	40.526144
3502.459143	360560.443926	40.531149
3504.578420	360812.404323	40.536154
3506.482415	361008.875022	40.541159
3508.362151	361162.142171	40.546164
3509.779358	361283.013478	40.551168
3510.943772	361365.501793	40.556173
3512.196093	361417.492437	40.561178
3512.834294	361441.844593	40.566183
3513.935747	361438.973237	40.571188
3514.837868	361418.118022	40.576192
3515.365835	361373.275983	40.581197
3515.255961	361314.030801	40.586202
3516.004496	361234.853221	40.591207
3516.039728	361159.223422	40.596212
3516.463419	361048.747918	40.601216
3516.514735	360939.297960	40.606221
3516.299066	360827.421719	40.611226
3516.339830	360706.242401	40.616231
3516.556127	360588.724681	40.621236
3516.854496	360436.307295	40.626240
3516.262219	360319.272980	40.631245
3516.142683	360174.503743	40.636250
3516.185267	360024.110284	40.641255
3515.666516	359895.841551	40.646260
3515.389066	359742.138901	40.651264
3515.352777	359594.708351	40.656269
3515.009410	359475.367915	40.661274
3514.839018	359343.403807	40.666279
3514.506903	359212.686345	40.671284
3514.438454	359067.371350	40.676288
3513.834033	358940.411421	40.681293
3513.699164	358809.432678	40.686298
3513.560956	358680.362630	40.691303
3512.735098	358556.948383	40.696308
3512.838719	358435.651675	40.701312
3513.124871	358335.752246	40.706317
3512.316392	358210.578536	40.711322
3512.458441	358093.422794	40.716327
3512.064386	357987.904573	40.721332
3511.949167	357871.883208	40.726336
3511.690144	357777.209188	40.731341
3511.471979	357678.584183	40.736346
3511.318777	357564.680239	40.741351
3510.604222	357479.264195	40.746356
3510.591251	357392.261139	40.751360
3510.495940	357297.102270	40.756365
3510.269686	357210.107165	40.761370
3510.189126	357125.353721	40.766375
3509.900254	357051.346555	40.771380
3509.813588	356954.429775	40.776384
3509.616929	356881.807409	40.781389
3509.538421	356804.025795	40.786394
3509.368419	356729.439510	40.791399
3509.429108	356650.515948	40.796404
3509.102649	356571.729807	40.801408
3509.163561	356509.474402	40.806413
3508.754313	356438.335538	40.811418
3508.870915	356369.810940	40.816423
3508.364178	356305.914551	40.821428
3508.350584	356233.084174	40.826432
3508.240686	356177.039257	40.831437
3508.227199	356121.055381	40.836442
3508.077785	356065.042036	40.841447
3507.777418	356007.830976	40.846452
3507.704097	355948.649889	40.851456
3507.770112	355896.928509	40.856461
3507.507960	355840.398323	40.861466
3507.675939	355801.741167	40.866471
3507.498720	355750.694298	40.871476
3507.219153	355709.842917	40.876480
3507.163602	355649.564393	40.881485
3507.019361	355616.580555	40.886490
3507.101613	355564.194611	40.891495
3506.932383	355517.421588	40.896500
3506.721736	355491.828229	40.901504
3506.623601	355448.199518	40.906509
3506.528683	355413.553598	40.911514
3506.703834	355369.067264	40.916519
3506.160819	355335.586417	40.921524
3506.153416	355303.140614	40.926528
3506.284108	355261.765943	40.931533
3506.104890	355254.694089	40.936538
3506.299029	355223.641497	40.941543
3506.049339	355199.886467	40.946548
3505.987221	355167.194741	40.951552
3506.041773	355144.180497	40.956557
3506.170248	355111.204119	40.961562
3506.058884	355076.280634	40.966567
3505.873984	355055.772730	40.971572
3506.081968	355015.708976	40.976576
3506.263197	354997.917081	40.981581
3505.763031	354966.286978	40.986586
3506.065312	354933.893779	40.991591
3505.967602	354909.147535	40.996596
3505.749377	354888.110407	41.001600
3505.443454	354862.633591	41.006605
3505.688837	354840.861485	41.011610
3505.645892	354811.245809	41.016615
3505.904437	354790.947634	41.021620
3505.644207	354764.267450	41.026624
3505.766307	354744.728844	41.031629
3505.661618	354726.778464	41.036634
3505.583118	354689.304634	41.041639
3505.498411	354665.014297	41.046644
3505.452989	354650.490124	41.051648
3505.470936	354630.026330	41.056653
3505.449599	354622.471349	41.061658
3505.612700	354589.311020	41.066663
3505.211861	354574.741217	41.071668
3505.383110	354556.950748	41.076672
3505.586701	354532.360283	41.081677
3505.141920	354515.710593	41.086682
3505.398499	354500.909596	41.091687
3505.232864	354484.597502	41.096692
3505.054547	354457.267985	41.101696
3505.339440	354448.697506	41.106701
3505.128520	354422.263840	41.111706
3505.606200	354405.671879	41.116711
3505.207226	354395.835252	41.121716
3504.905815	354359.745222	41.126720
3505.209636	354353.360354	41.131725
3504.974552	354349.681932	41.136730
3505.094228	354326.886070	41.141735
3505.081257	354326.811753	41.146740
3504.962294	354302.144924	41.151744
3504.956589	354292.322455	41.156749
3504.972419	354277.584902	41.161754
3505.210934	354252.988783	41.166759
3505.115100	354246.819777	41.171764
3504.694549	354220.546394	41.176768
3505.161518	354201.283902	41.181773
3505.361871	354198.605497	41.186778
3505.186766	354168.297770	41.191783
3505.225994	354161.572970	41.196788
3505.470800	354138.782693	41.201792
3505.140370	354115.167173	41.206797
3505.077053	354098.151655	41.211802
3504.980487	354079.232697	41.216807
3504.969990	354074.780725	41.221812
3504.893818	354057.716327	41.226816
3505.166123	354033.572849	41.231821
3504.749097	354027.785432	41.236826
3504.442459	354007.805341	41.241831
3504.867620	353995.827864	41.246836
3505.023527	353991.833115	41.251840
3504.640094	353973.570250	41.256845
3504.981051	353956.897963	41.261850
3505.166684	353941.878979	41.266855
3504.743929	353932.173270	41.271860
3504.696050	353927.040065	41.276864
3504.985835	353912.946230	41.281869
3504.719585	353899.169337	41.286874
3504.900690	353879.671976	41.291879
3504.793802	353870.094466	41.296884
3504.742417	353854.527592	41.301888
3504.552556	353842.800002	41.306893
3504.437117	353836.099611	41.311898
3504.786045	353828.765923	41.316903
3504.658575	353815.730549	41.321908
3504.459844	353804.844180	41.326912
3504.508588	353807.635881	41.331917
3504.728804	353796.276092	41.336922
3504.784406	353783.008173	41.341927
3504.563522	353767.264474	41.346932
3504.741850	353755.122368	41.351936
3504.701611	353744.083685	41.356941
3504.565275	353733.772773	41.361946
3505.069423	353725.574704	41.366951
3504.794993	353711.595459	41.371956
3504.922737	353703.660486	41.376960
3505.012133	353680.131096	41.381965
3504.960114	353664.895108	41.386970
3504.658470	353651.836328	41.391975
3504.742516	353632.634162	41.396980
3504.913722	353618.686241	41.401984
3504.771574	353607.103752	41.406989
3504.558254	353596.906782	41.411994
3505.207463	353592.528624	41.416999
3504.850459	353571.385654	41.422004
3504.715248	353569.447400	41.427008
3504.738911	353542.212720	41.432013
3504.538211	353534.940430	41.437018
3504.568090	353523.483424	41.442023
3504.609585	353520.880997	41.447028
3504.611666	353510.599059	41.452032
3504.518217	353498.296262	41.457037
3504.150925	353483.924445	41.462042
3504.522471	353468.774137	41.467047
3504.692514	353472.335614	41.472052
3504.495044	353469.618265	41.477056
3504.507195	353447.856997	41.482061
3504.456814	353438.957611	41.487066
3504.280326	353439.723527	41.492071
3504.326852	353435.796926	41.497076
3504.662932	353422.102833	41.502080
3504.578080	353410.002252	41.507085
3504.218083	353406.623456	41.512090
3504.699791	353396.520168	41.517095
3504.606720	353384.904422	41.522100
3504.559476	353376.920714	41.527104
3504.266518	353353.222576	41.532109
3504.480262	353349.778524	41.537114
3504.733538	353336.199298	41.542119
3504.609847	353335.073600	41.547124
3504.782452	353323.415841	41.552128
3504.720601	353298.510463	41.557133
3504.192584	353305.312604	41.562138
3504.658409	353295.339056	41.567143
3504.317046	353278.214528	41.572148
3504.285660	353281.477017	41.577152
3504.541396	353260.389752	41.582157
3504.251294	353262.598808	41.587162
3504.773776	353245.515855	41.592167
3504.302892	353248.898724	41.597172
3504.576476	353232.262307	41.602176
3504.620155	353221.312046	41.607181
3504.281203	353211.872900	41.612186
3504.176201	353196.288857	41.617191
3504.559531	353197.297121	41.622196
3504.391421	353180.959561	41.627200
3504.662104	353178.168188	41.632205
3504.317600	353163.283688	41.637210
3504.863999	353153.424623	41.642215
3504.442918	353147.485052	41.647220
3504.321899	353142.312432	41.652224
3504.296225	353152.038238	41.657229
3504.303816	353151.044481	41.662234
3504.399931	353140.009565	41.667239
3504.624162	353135.164110	41.672244
3504.388769	353118.099127	41.677248
3504.512140	353107.339841	41.682253
3504.538054	353106.928529	41.687258
3504.734702	353098.524477	41.692263
3504.625055	353088.718213	41.697268
3504.443014	353066.402144	41.702272
3504.630401	353049.982894	41.707277
3504.575896	353051.111277	41.712282
3504.516994	353025.518162	41.717287
3504.523682	353020.223543	41.722292
3504.478559	353010.916059	41.727296
3504.465803	352996.029966	41.732301
3503.912292	353005.559296	41.737306
3504.295079	352992.901147	41.742311
3504.566081	352979.548074	41.747316
3504.436973	352972.773383	41.752320
3504.634464	352959.940921	41.757325
3504.394435	352957.459321	41.762330
3504.541333	352945.067499	41.767335
3504.597917	352916.453004	41.772340
3504.374162	352912.619991	41.777344
3504.546627	352916.919166	41.782349
3504.351665	352889.616910	41.787354
3504.511245	352883.203767	41.792359
3504.095714	352890.904370	41.797364
3504.323723	352872.773508	41.802368
3504.579304	352862.629517	41.807373
3504.084713	352862.249588	41.812378
3504.207790	352845.636843	41.817383
3504.207129	352842.659300	41.822388
3504.514004	352836.680962	41.827392
3504.407801	352831.735018	41.832397
3504.097513	352828.628274	41.837402
3504.510273	352822.836794	41.842407
3504.354363	352805.021099	41.847412
3504.317909	352802.736358	41.852416
3504.637114	352790.673558	41.857421
3504.452688	352774.491150	41.862426
3504.336100	352760.715748	41.867431
3504.028625	352772.242212	41.872436
3504.342287	352755.981058	41.877440
3504.500393	352751.171471	41.882445
3504.112646	352747.008073	41.887450
3504.163460	352743.513390	41.892455
3504.032068	352727.602533	41.897460
3503.949266	352730.033338	41.902464
3504.106860	352712.142602	41.907469
3503.849189	352719.385626	41.912474
3503.883272	352721.085358	41.917479
3503.981882	352717.608567	41.922484
3504.023040	352710.476078	41.927488
3504.346986	352698.158009	41.932493
3504.068813	352712.530239	41.937498
3504.252272	352698.910986	41.942503
3504.344259	352685.942438	41.947508
3504.318253	352672.865289	41.952512
3504.494284	352671.132298	41.957517
3504.169313	352660.036600	41.962522
3504.524312	352657.359120	41.967527
3504.080538	352655.571412	41.972532
3504.321730	352633.213702	41.977536
3504.397527	352603.832503	41.982541
3504.439329	352600.135636	41.987546
3504.487224	352587.835732	41.992551
3504.443961	352573.819640	41.997556
3504.015911	352586.001454	42.002560
3504.572404	352558.325733	42.007565
3504.371818	352554.030932	42.012570
3504.550558	352532.446551	42.017575
3504.448672	352531.037439	42.022580
3504.398737	352515.164540	42.027584
3504.333829	352520.086622	42.032589
3504.280513	352499.887761	42.037594
3504.363148	352482.823196	42.042599
3504.321922	352485.247440	42.047604
3504.311442	352463.133044	42.052608
3504.394400	352460.065911	42.057613
3504.159176	352462.902574	42.062618
3503.922685	352453.803394	42.067623
3503.999032	352434.296609	42.072628
3504.087756	352436.980262	42.077632
3504.202576	352431.617590	42.082637
3503.872278	352439.304784	42.087642
3504.342622	352426.887158	42.092647
3504.524805	352412.682684	42.097652
3503.921483	352412.650790	42.102656
3504.287891	352419.769747	42.107661
3504.100964	352397.301468	42.112666
3504.108945	352392.566482	42.117671
3503.724283	352384.992266	42.122676
3503.611571	352383.610312	42.127680
3504.161179	352380.851153	42.132685
3503.776827	352386.663598	42.137690
3504.272785	352383.938370	42.142695
3504.227183	352381.655056	42.147700
3503.945722	352392.821190	42.152704
3504.023363	352394.030496	42.157709
3504.177748	352386.040213	42.162714
3504.135930	352382.432899	42.167719
3504.084743	352377.274616	42.172724
3504.293707	352379.812013	42.177728
3504.388780	352370.355002	42.182733
3504.078598	352368.978816	42.187738
3504.066539	352354.296032	42.192743
3504.332155	352362.957933	42.197748
3504.459365	352340.083668	42.202752
3504.365841	352336.713576	42.207757
3504.343501	352332.568729	42.212762
3504.293037	352306.159531	42.217767
3504.225194	352302.301826	42.222772
3504.057904	352292.911729	42.227776
3504.276812	352300.537570	42.232781
3503.737192	352287.134322	42.237786
3503.975246	352276.458538	42.242791
3504.202704	352271.128944	42.247796
3503.827318	352286.661910	42.252800
3504.330075	352276.784133	42.257805
3504.168967	352260.546982	42.262810
3504.328060	352252.352334	42.267815
3504.096037	352254.119598	42.272820
3504.139249	352255.843352	42.277824
3504.169792	352224.483991	42.282829
3503.762736	352235.720912	42.287834
3503.962082	352226.374642	42.292839
3503.998554	352228.862965	42.297844
3503.949925	352226.758274	42.302848
3503.973576	352211.509904	42.307853
3503.759578	352211.161962	42.312858
3503.895917	352203.429005	42.317863
3503.839442	352205.652071	42.322868
3504.321663	352213.032699	42.327872
3504.335566	352198.065817	42.332877
3503.880043	352187.626911	42.337882
3504.436031	352170.792817	42.342887
3504.245138	352177.007354	42.347892
3504.117027	352168.094592	42.352896
3504.268993	352146.132535	42.357901
3503.931966	352155.195141	42.362906
3504.163881	352155.082107	42.367911
3504.304256	352150.682472	42.372916
3503.805737	352136.101982	42.377920
3503.904590	352125.957177	42.382925
3503.983012	352134.801408	42.387930
3503.887893	352126.290626	42.392935
3504.010356	352137.062106	42.397940
3504.010195	352121.359372	42.402944
3504.076833	352098.927232	42.407949
3503.884480	352112.395301	42.412954
3503.984555	352101.028691	42.417959
3504.119739	352112.052666	42.422964
3504.024385	352106.417786	42.427968
3504.284605	352083.573284	42.432973
3503.921377	352083.834286	42.437978
3504.128337	352084.997705	42.442983
3503.844948	352085.856890	42.447988
3503.991413	352073.490384	42.452992
3503.980299	352054.226337	42.457997
3503.726732	352057.142272	42.463002
3503.929072	352057.746518	42.468007
3503.870477	352071.371604	42.473012
3503.900830	352073.682750	42.478016
3504.261559	352059.170004	42.483021
3504.061252	352040.597567	42.488026
3504.271900	352042.473009	42.493031
3504.155492	352054.249375	42.498036
3504.140603	352035.036819	42.503040
3504.624210	352011.342566	42.508045
3504.019385	352017.368056	42.513050
3503.998385	352011.823212	42.518055
3503.914950	351999.467582	42.523060
3503.828805	351994.365688	42.528064
3504.133780	351983.704717	42.533069
3503.977452	351986.681634	42.538074
3504.104975	351994.194716	42.543079
3504.349846	351983.899549	42.548084
3504.055786	351973.842280	42.553088
3504.143565	351973.548430	42.558093
3504.048433	351974.505106	42.563098
3504.034497	351956.997536	42.568103
3504.051550	351941.037525	42.573108
3504.052795	351946.509108	42.578112
3504.169228	351938.702909	42.583117
3504.263751	351937.008230	42.588122
3503.787269	351919.904623	42.593127
3503.908300	351918.358454	42.598132
3503.851708	351918.240128	42.603136
3504.550894	351912.454171	42.608141
3503.808322	351918.068794	42.613146
3504.215260	351897.160687	42.618151
3503.832731	351888.873455	42.623156
3503.942915	351895.574883	42.628160
3504.183060	351893.068224	42.633165
3503.930211	351903.084674	42.638170
3503.747715	351879.572016	42.643175
3503.966047	351876.101694	42.648180
3503.985444	351862.889918	42.653184
3504.451676	351866.150177	42.658189
3504.276344	351878.394002	42.663194
3504.294707	351855.409486	42.668199
3504.102018	351831.593014	42.673204
3504.022488	351847.333840	42.678208
3504.124260	351845.994316	42.683213
3503.807216	351823.520914	42.688218
3504.006621	351817.864856	42.693223
3504.009248	351823.132630	42.698228
3504.076138	351815.436047	42.703232
3504.235658	351817.930387	42.708237
3503.981811	351795.446983	42.713242
3503.829951	351766.457616	42.718247
3504.206172	351783.271677	42.723252
3503.811947	351793.335948	42.728256
3504.043660	351778.410867	42.733261
3503.879801	351785.868240	42.738266
3504.020806	351769.175974	42.743271
3504.053687	351758.837926	42.748276
3504.125516	351751.216904	42.753280
3504.152845	351758.109600	42.758285
3504.024998	351749.425780	42.763290
3503.874617	351725.755275	42.768295
3504.024054	351726.520591	42.773300
3503.961931	351730.373391	42.778304
3504.093844	351718.009103	42.783309
3503.772932	351717.143602	42.788314
3503.857377	351692.926953	42.793319
3503.855548	351682.899782	42.798324
3503.772818	351689.631733	42.803329
3503.973629	351687.513038	42.808333
3503.840710	351686.516016	42.813338
3503.905294	351685.462320	42.818343
3503.797660	351695.913959	42.823348
3503.857784	351682.721151	42.828353
3503.919970	351664.514291	42.833357
3503.863202	351658.364256	42.838362
3504.020186	351657.143251	42.843367
3504.019735	351670.224789	42.848372
3503.613235	351673.063120	42.853377
3504.103085	351665.732307	42.858381
3504.000210	351650.707382	42.863386
3503.843016	351643.657008	42.868391
3504.022460	351646.199107	42.873396
3503.794662	351645.344335	42.878401
3504.296322	351650.355083	42.883405
3504.058592	351637.463853	42.888410
3503.952159	351619.639941	42.893415
3503.927896	351619.669206	42.898420
3503.734674	351621.226754	42.903425
3504.092908	351621.831811	42.908429
3503.768158	351623.002946	42.913434
3504.007745	351599.296187	42.918439
3504.098216	351591.773996	42.923444
3503.803392	351591.693331	42.928449
3503.991945	351589.881975	42.933453
3503.942702	351610.122803	42.938458
3504.001990	351597.566365	42.943463
3503.922935	351571.644882	42.948468
3503.599648	351568.082010	42.953473
3503.832434	351569.165007	42.958477
3503.762118	351579.763471	42.963482
3503.947798	351577.265408	42.968487
3503.980956	351577.845504	42.973492
3503.627288	351578.741257	42.978497
3503.944995	351579.021866	42.983501
3503.614014	351571.998956	42.988506
3503.864842	351555.823721	42.993511
3503.854408	351559.464759	42.998516
3503.814628	351564.739262	43.003521
3504.031750	351563.101541	43.008525
3503.989319	351571.761368	43.013530
3503.928780	351567.546149	43.018535
3504.073224	351548.791788	43.023540
3504.157631	351545.418968	43.028545
3504.007820	351533.480931	43.033549
3503.756303	351553.448352	43.038554
3503.543419	351538.186283	43.043559
3503.972231	351554.050436	43.048564
3504.009203	351526.176356	43.053569
3504.247777	351524.789747	43.058573
3503.884895	351528.308352	43.063578
3503.995502	351516.100088	43.068583
3504.187801	351526.249840	43.073588
3503.869057	351504.463735	43.078593
3504.108228	351478.237395	43.083597
3503.934576	351485.416403	43.088602
3504.237031	351486.132081	43.093607
3503.983414	351484.085217	43.098612
3503.866151	351464.405082	43.103617
3504.114119	351458.232300	43.108621
3504.041468	351449.692408	43.113626
3504.013959	351452.750792	43.118631
3503.868230	351459.823587	43.123636
3503.828530	351445.450330	43.128641
3504.116777	351426.749544	43.133645
3503.848256	351425.239494	43.138650
3503.934477	351431.715714	43.143655
3503.951152	351422.627237	43.148660
3503.899645	351430.550457	43.153665
3504.107970	351418.937535	43.158669
3503.749691	351402.883996	43.163674
3503.918072	351410.848809	43.168679
3503.775952	351395.448260	43.173684
3503.742474	351410.698374	43.178689
3503.991110	351411.702517	43.183693
3503.825938	351411.703157	43.188698
3503.809692	351383.837417	43.193703
3503.921858	351377.457039	43.198708
3503.816437	351385.185185	43.203713
3503.848861	351376.170562	43.208717
3503.575406	351386.546673	43.213722
3503.673624	351389.330680	43.218727
3503.531335	351389.302252	43.223732
3503.562994	351392.783944	43.228737
3503.804230	351386.103208	43.233741
3504.070900	351388.758782	43.238746
3504.068748	351379.851428	43.243751
3504.394212	351376.567741	43.248756
3503.889748	351373.517058	43.253761
3504.151735	351362.481002	43.258765
3504.050829	351356.439712	43.263770
3504.023362	351348.096266	43.268775
3504.069284	351327.448614	43.273780
3503.871694	351343.182801	43.278785
3503.933548	351334.927033	43.283789
3503.865596	351347.612112	43.288794
3503.820403	351334.003209	43.293799
3503.809381	351315.858706	43.298804
3503.761794	351314.695484	43.303809
3503.808403	351313.161063	43.308813
3503.741636	351312.713487	43.313818
3504.070006	351310.065601	43.318823
3503.898920	351313.986558	43.323828
3503.717470	351318.494515	43.328833
3504.067107	351301.260112	43.333837
3503.686469	351298.927914	43.338842
3503.904289	351289.934869	43.343847
3503.759989	351282.246146	43.348852
3503.617145	351288.096881	43.353857
3503.827233	351293.968174	43.358861
3503.746099	351288.203706	43.363866
3504.008371	351291.852552	43.368871
3503.800215	351288.322362	43.373876
3503.671727	351283.761556	43.378881
3503.982643	351272.285087	43.383885
3503.822228	351279.563832	43.388890
3504.021842	351277.368958	43.393895
3504.126907	351268.520987	43.398900
3504.023246	351266.654013	43.403905
3504.112742	351250.529641	43.408909
3504.167004	351231.102261	43.413914
3504.133039	351247.090565	43.418919
3503.786763	351239.306512	43.423924
3504.116590	351232.560851	43.428929
3504.045998	351212.084278	43.433933
3503.906019	351209.815834	43.438938
3503.939823	351220.754217	43.443943
3504.225773	351207.423790	43.448948
3503.981925	351214.512129	43.453953
3503.790182	351186.114117	43.458957
3503.798693	351184.356660	43.463962
3503.942414	351189.373136	43.468967
3503.912322	351198.234676	43.473972
3503.695377	351201.093967	43.478977
3504.115261	351181.354263	43.483981
3503.901809	351183.958496	43.488986
3503.841220	351169.741170	43.493991
3504.230333	351163.240634	43.498996
3503.871680	351166.020526	43.504001
3504.093943	351164.152925	43.509005
3503.724144	351175.002418	43.514010
3503.760789	351148.884286	43.519015
3503.776947	351139.948547	43.524020
3503.844911	351145.740521	43.529025
3504.107335	351136.562245	43.534029
3503.688149	351144.136422	43.539034
3503.930985	351149.518992	43.544039
3503.625722	351146.360453	43.549044
3503.492484	351140.807811	43.554049
3504.012775	351139.631163	43.559053
3503.916325	351131.247686	43.564058
3503.894683	351117.227795	43.569063
3503.867917	351116.010376	43.574068
3503.543584	351127.259901	43.579073
3504.290369	351120.524662	43.584077
3503.906548	351124.275658	43.589082
3503.578670	351123.258545	43.594087
3503.774026	351106.099370	43.599092
3503.963086	351102.888133	43.604097
3504.263865	351097.954042	43.609101
3503.840358	351092.549085	43.614106
3503.867779	351090.483228	43.619111
3503.819247	351096.420877	43.624116
3503.699300	351097.814153	43.629121
3503.912722	351079.735891	43.634125
3503.819179	351074.507826	43.639130
3504.010897	351064.119084	43.644135
3503.935013	351071.817155	43.649140
3503.564975	351068.541598	43.654145
3503.660775	351067.432054	43.659149
3503.715199	351078.621713	43.664154
3504.115176	351078.965671	43.669159
3504.138789	351069.443377	43.674164
3503.847982	351055.720528	43.679169
3503.909513	351043.545367	43.684173
3503.707480	351052.154155	43.689178
3503.691427	351050.451478	43.694183
3503.649568	351053.206746	43.699188
3503.662959	351057.912978	43.704193
3504.064763	351041.001104	43.709197
3503.564282	351036.957196	43.714202
3503.803855	351022.717831	43.719207
3503.871043	351012.679624	43.724212
3503.482552	351026.026268	43.729217
3503.847698	351007.338632	43.734221
3503.666692	351019.990759	43.739226
3503.904485	351023.567141	43.744231
3503.997458	351029.889638	43.749236
3504.090805	351024.937431	43.754241
3503.897487	351015.932984	43.759245
3503.662207	351010.040151	43.764250
3503.847857	350991.838997	43.769255
3503.647248	351001.440146	43.774260
3503.537024	351006.369530	43.779265
3503.685145	351014.795717	43.784269
3503.773784	351022.645940	43.789274
3504.147544	351006.654712	43.794279
3504.121289	351023.558088	43.799284
3503.857242	351007.082324	43.804289
3504.184365	350976.718827	43.809293
3504.084786	350976.225534	43.814298
3504.372408	350974.220341	43.819303
3504.289901	350954.789032	43.824308
3504.291659	350943.106861	43.829313
3504.302689	350937.531392	43.834317
3504.064377	350922.374971	43.839322
3504.320518	350910.118113	43.844327
3504.028391	350909.731611	43.849332
3503.633232	350910.506680	43.854337
3503.958472	350908.190128	43.859341
3503.444440	350913.972331	43.864346
3503.784298	350909.032044	43.869351
3503.897573	350880.814710	43.874356
3503.529838	350879.091272	43.879361
3503.722917	350879.238883	43.884365
3503.747218	350876.231834	43.889370
3503.876177	350875.269749	43.894375
3504.108980	350876.327306	43.899380
3503.983209	350883.397022	43.904385
3503.922972	350876.203966	43.909389
3503.543818	350870.995581	43.914394
3503.854095	350860.486255	43.919399
3504.033408	350862.595750	43.924404
3503.825135	350864.282952	43.929409
3503.987532	350854.229665	43.934413
3503.773741	350863.018498	43.939418
3503.660560	350852.270704	43.944423
3503.764145	350850.701812	43.949428
3503.641386	350832.422107	43.954433
3503.949273	350826.163428	43.959437
3503.687544	350836.410537	43.964442
3503.763500	350830.722990	43.969447
3503.806759	350817.888947	43.974452
3503.723541	350835.437655	43.979457
3503.899364	350832.126691	43.984461
3503.682486	350839.923436	43.989466
3504.094961	350828.888932	43.994471
3504.094007	350809.979146	43.999476
3503.980947	350811.015029	44.004481
3504.175265	350804.876104	44.009485
3504.055205	350815.889795	44.014490
3504.051453	350794.918933	44.019495
3504.155292	350770.291592	44.024500
3503.942412	350774.550055	44.029505
3503.980836	350770.929948	44.034509
3503.823929	350778.564517	44.039514
3503.966361	350764.747653	44.044519
3503.885714	350768.323492	44.049524
3503.677904	350757.972401	44.054529
3503.851862	350747.408251	44.059533
3503.830610	350764.921735	44.064538
3504.232338	350759.462639	44.069543
3504.382233	350756.384826	44.074548
3503.920871	350739.049396	44.079553
3504.023764	350731.601475	44.084557
3503.776301	350724.641603	44.089562
3503.847234	350729.084260	44.094567
3503.730555	350726.786661	44.099572
3503.637612	350728.837398	44.104577
3503.747605	350728.896341	44.109581
3503.640816	350729.880332	44.114586
3503.541255	350709.204542	44.119591
3503.967068	350700.636633	44.124596
3503.760748	350701.254598	44.129601
3503.698504	350698.363023	44.134605
3503.462644	350704.686641	44.139610
3503.745800	350696.217636	44.144615
3503.616010	350697.408871	44.149620
3503.545694	350705.487876	44.154625
3503.776808	350700.284802	44.159629
3503.606038	350699.319196	44.164634
3503.852414	350707.526291	44.169639
3503.866103	350704.851771	44.174644
3503.872618	350720.604773	44.179649
3503.845874	350693.529312	44.184653
3503.699987	350694.544936	44.189658
3503.558602	350676.140869	44.194663
3503.605816	350676.209736	44.199668
3503.510634	350687.321323	44.204673
3503.548425	350681.512540	44.209677
3503.713819	350683.293381	44.214682
3503.425797	350691.177747	44.219687
3503.971045	350690.607963	44.224692
3503.759522	350695.960603	44.229697
3503.983396	350696.688716	44.234701
3503.535268	350702.765931	44.239706
3503.784550	350691.451789	44.244711
3503.889803	350676.648199	44.249716
3503.594330	350666.845416	44.254721
3503.909504	350652.695806	44.259725
3503.753382	350667.329247	44.264730
3503.966216	350670.298778	44.269735
3504.122838	350670.884817	44.274740
3503.924913	350669.490839	44.279745
3504.035663	350658.325844	44.284749
3503.783652	350645.029422	44.289754
3503.778065	350647.626270	44.294759
3504.059630	350633.380165	44.299764
3503.695783	350647.181121	44.304769
3504.036423	350642.317040	44.309773
3504.082579	350641.469844	44.314778
3503.965661	350630.086326	44.319783
3503.899192	350609.659775	44.324788
3503.544690	350603.633041	44.329793
3503.539468	350606.306186	44.334797
3503.634087	350615.173557	44.339802
3503.700451	350616.461039	44.344807
3503.905768	350609.404123	44.349812
3503.655394	350625.121411	44.354817
3504.045997	350614.472085	44.359821
3503.910017	350596.067136	44.364826
3504.140120	350585.468627	44.369831
3503.975514	350587.759756	44.374836
3503.559845	350594.417223	44.379841
3504.048928	350589.504219	44.384845
3504.043055	350582.455235	44.389850
3504.000684	350567.089582	44.394855
3504.128284	350553.071403	44.399860
3503.794229	350548.186719	44.404865
3503.938340	350559.540463	44.409869
3504.229833	350552.928032	44.414874
3504.238718	350534.856473	44.419879
3504.076527	350526.559649	44.424884
3503.869863	350528.959233	44.429889
3504.093008	350511.897282	44.434893
3503.615701	350516.833840	44.439898
3503.556270	350526.056441	44.444903
3503.738497	350507.372099	44.449908
3503.659750	350492.953860	44.454913
3503.741665	350483.905813	44.459917
3503.471445	350488.122462	44.464922
3503.822394	350480.864350	44.469927
3503.696736	350490.911856	44.474932
3503.751328	350504.366738	44.479937
3504.012214	350496.257535	44.484941
3503.805727	350494.610397	44.489946
3503.996823	350492.722249	44.494951
3504.211026	350489.837863	44.499956
3504.049378	350470.011678	44.504961
3504.032133	350470.116187	44.509965
3503.664776	350469.079851	44.514970
3503.751685	350456.875095	44.519975
3503.952385	350468.779832	44.524980
3503.486947	350472.111110	44.529985
3503.832374	350459.992741	44.534989
3503.676177	350458.363103	44.539994
3503.598147	350438.447334	44.544999
3503.857848	350438.431708	44.550004
3503.723123	350436.391460	44.555009
3503.862901	350426.596179	44.560013
3503.695125	350438.101057	44.565018
3503.886327	350422.825694	44.570023
3504.150958	350446.834979	44.575028
3503.522646	350444.363741	44.580033
3503.738681	350416.028117	44.585037
3503.769101	350415.717876	44.590042
3503.533422	350409.799590	44.595047
3503.924629	350413.351760	44.600052
3503.785981	350415.995105	44.605057
3503.874831	350407.149558	44.610061
3503.480625	350422.227917	44.615066
3503.754916	350416.483522	44.620071
3503.596812	350413.963400	44.625076
3503.706613	350410.535593	44.630081
3503.958527	350413.498960	44.635085
3503.811884	350405.581424	44.640090
3503.705688	350389.920400	44.645095
3503.606315	350391.005029	44.650100
3503.681016	350389.109828	44.655105
3503.665375	350388.043339	44.660109
3503.530331	350391.525998	44.665114
3503.718588	350393.939508	44.670119
3503.701477	350386.281452	44.675124
3503.678763	350398.450582	44.680129
3503.748017	350402.918982	44.685133
3503.639161	350401.994485	44.690138
3503.729883	350399.129614	44.695143
3504.123858	350404.157503	44.700148
3503.977194	350379.264175	44.705153
3503.970746	350371.197215	44.710157
3503.777899	350369.038898	44.715162
3503.750336	350367.770686	44.720167
3503.854929	350372.233501	44.725172
3503.386068	350372.562111	44.730177
3503.923265	350377.261948	44.735181
3503.856460	350369.942609	44.740186
3503.620798	350371.557803	44.745191
3503.585718	350350.184507	44.750196
3503.499041	350342.741051	44.755201
3503.681632	350354.368715	44.760205
3503.574356	350361.130162	44.765210
3503.516237	350345.690584	44.770215
3503.858644	350357.674747	44.775220
3503.704718	350362.051177	44.780225
3503.708996	350359.149068	44.785229
3503.616246	350362.166926	44.790234
3503.494535	350368.752497	44.795239
3503.677863	350362.258947	44.800244
3503.692559	350365.616131	44.805249
3503.778158	350355.396737	44.810253
3503.438988	350379.679662	44.815258
3503.471722	350371.453802	44.820263
3503.639137	350367.024297	44.825268
3503.410412	350383.323605	44.830273
3503.539653	350372.486491	44.835277
3503.631592	350379.114638	44.840282
3503.373791	350381.522313	44.845287
3503.689047	350379.843592	44.850292
3503.692371	350390.354295	44.855297
3503.580744	350398.668934	44.860301
3503.424299	350406.863403	44.865306
3503.816114	350406.343323	44.870311
3503.770236	350400.700443	44.875316
3503.684160	350382.898355	44.880321
3504.065028	350363.062719	44.885325
3504.096132	350382.502323	44.890330
3503.837641	350378.394659	44.895335
3503.813403	350377.125921	44.900340
3503.770469	350384.029900	44.905345
3503.952608	350371.148346	44.910349
3503.833464	350361.877554	44.915354
3503.684692	350356.556347	44.920359
3503.976889	350353.914133	44.925364
3503.394052	350355.609664	44.930369
3503.965450	350353.839547	44.935373
3503.616366	350353.462045	44.940378
3503.766730	350359.750097	44.945383
3503.744243	350357.717552	44.950388
3503.729992	350357.694333	44.955393
3503.731570	350345.655749	44.960397
3503.453657	350331.294403	44.965402
3503.213876	350327.183777	44.970407
3503.807917	350331.416515	44.975412
3504.016312	350334.183158	44.980417
3503.904782	350325.343824	44.985421
3503.617822	350330.988386	44.990426
3504.074542	350320.939374	44.995431
3503.799198	350322.840804	45.000436
3503.756247	350322.211298	45.005441
3504.008342	350328.050604	45.010445
3503.595614	350310.096524	45.015450
3503.729469	350315.572758	45.020455
3504.026951	350296.106594	45.025460
3504.008080	350300.563483	45.030465
3504.030525	350296.589557	45.035469
3503.808314	350301.129493	45.040474
3503.661473	350302.959707	45.045479
3503.587271	350262.758815	45.050484
3503.612734	350277.516360	45.055489
3503.830306	350255.670418	45.060493
3503.779227	350276.802820	45.065498
3503.733879	350271.617961	45.070503
3503.597319	350272.988432	45.075508
3503.674098	350276.132200	45.080513
3503.764857	350280.139091	45.085517
3503.757069	350275.991786	45.090522
3504.226481	350273.168847	45.095527
3503.777476	350266.088072	45.100532
3503.601520	350254.713809	45.105537
3503.490041	350243.278448	45.110541
3503.617770	350239.771443	45.115546
3503.651007	350250.939171	45.120551
3504.056395	350255.049031	45.125556
3503.693583	350248.387295	45.130561
3503.650938	350246.663346	45.135565
3503.589509	350253.875677	45.140570
3503.763735	350250.463127	45.145575
3503.676243	350260.631897	45.150580
3503.566641	350254.540957	45.155585
3503.964012	350253.790939	45.160589
3503.828922	350254.194039	45.165594
3503.528293	350237.087549	45.170599
3503.814343	350221.084506	45.175604
3503.662954	350224.137092	45.180609
3503.684034	350225.380839	45.185613
3503.805610	350219.227898	45.190618
3503.739469	350219.721903	45.195623
3503.599289	350217.758861	45.200628
3503.598846	350237.127151	45.205633
3503.945881	350230.760412	45.210637
3503.776716	350228.623795	45.215642
3503.468414	350237.631278	45.220647
3503.956900	350229.842370	45.225652
3503.338291	350218.970744	45.230657
3503.629123	350206.428283	45.235661
3503.554852	350204.123958	45.240666
3503.625819	350200.956788	45.245671
3503.720727	350201.196273	45.250676
3503.465252	350208.897406	45.255681
3503.836645	350195.858637	45.260685
3503.697909	350206.824500	45.265690
3503.947741	350207.904830	45.270695
3503.760651	350210.250431	45.275700
3503.744792	350214.554144	45.280705
3504.168483	350209.829602	45.285709
3503.690303	350203.491511	45.290714
3503.550090	350181.422139	45.295719
3503.916675	350181.338715	45.300724
3503.418732	350181.010196	45.305729
3503.563994	350179.281990	45.310733
3503.789245	350185.481869	45.315738
3503.353410	350191.200883	45.320743
3503.676654	350186.237707	45.325748
3503.710010	350182.109342	45.330753
3503.714287	350194.325152	45.335757
3503.686635	350196.340136	45.340762
3503.769528	350195.258066	45.345767
3503.821766	350182.676965	45.350772
3503.810727	350199.832701	45.355777
3504.046831	350184.550173	45.360781
3503.751044	350161.996367	45.365786
3503.774384	350158.556762	45.370791
3503.843028	350162.058137	45.375796
3503.883309	350156.885181	45.380801
3503.929725	350159.422929	45.385805
3503.703848	350157.549786	45.390810
3503.806992	350172.396884	45.395815
3503.917768	350147.335497	45.400820
3503.468759	350135.851668	45.405825
3503.742516	350125.246170	45.410829
3503.477071	350126.637020	45.415834
3503.513467	350122.940838	45.420839
3503.338880	350135.948470	45.425844
3503.452649	350130.916601	45.430849
3503.744131	350138.174961	45.435853
3503.699408	350128.892365	45.440858
3503.907084	350137.156566	45.445863
3503.888857	350117.333031	45.450868
3503.721854	350130.186759	45.455873
3503.891527	350133.672165	45.460877
3504.125993	350137.249131	45.465882
3504.181531	350123.445843	45.470887
3504.007436	350107.362803	45.475892
3503.842382	350104.665608	45.480897
3504.058650	350103.689707	45.485901
3503.861948	350108.632844	45.490906
3503.504776	350099.094224	45.495911
3503.834392	350073.769148	45.500916
3503.755665	350071.287364	45.505921
3503.807805	350075.860300	45.510925
3503.807606	350070.922795	45.515930
3503.900133	350069.101118	45.520935
3504.139147	350079.014696	45.525940
3503.747063	350072.612077	45.530945
3503.712003	350068.214556	45.535949
3503.342468	350054.732960	45.540954
3503.280569	350050.059718	45.545959
3503.906530	350073.324866	45.550964
3503.243928	350061.085804	45.555969
3503.440117	350071.006154	45.560973
3503.924331	350072.838418	45.565978
3503.930457	350067.136380	45.570983
3503.907353	350057.850354	45.575988
3503.529266	350069.923030	45.580993
3503.535459	350061.599516	45.585997
3503.681766	350062.696215	45.591002
3503.404996	350056.682582	45.596007
3503.722730	350060.068232	45.601012
3503.527170	350060.760856	45.606017
3503.877262	350059.840152	45.611021
3503.704401	350070.862340	45.616026
3503.452752	350065.837330	45.621031
3503.769373	350069.019546	45.626036
3503.524863	350078.373286	45.631041
3503.700287	350057.399266	45.636045
3503.641781	350052.623684	45.641050
3503.239943	350045.255461	45.646055
3503.630379	350049.342250	45.651060
3503.799217	350055.983732	45.656065
3503.672703	350039.613188	45.661069
3503.442787	350037.562522	45.666074
3503.635840	350041.527808	45.671079
3503.772728	350041.149831	45.676084
3503.357933	350036.405121	45.681089
3503.599126	350033.567347	45.686093
3503.953321	350040.917610	45.691098
3503.734609	350034.487579	45.696103
3503.951603	350046.898854	45.701108
3503.659944	350048.955580	45.706113
3503.963023	350045.573549	45.711117
3503.591109	350054.591118	45.716122
3503.741289	350043.521568	45.721127
3503.676736	350030.271715	45.726132
3503.488849	350027.527223	45.731137
3503.707331	350021.308037	45.736141
3503.754691	350034.382411	45.741146
3503.469597	350029.642648	45.746151
3503.794445	350026.028114	45.751156
3503.954485	350030.253132	45.756161
3503.951602	350033.791274	45.761165
3503.854472	350030.217999	45.766170
3503.737100	350034.639578	45.771175
3503.715148	350024.869793	45.776180
3503.529013	350006.243514	45.781185
3504.016440	349997.538499	45.786189
3503.772250	349988.770985	45.791194
3503.891708	350005.982505	45.796199
3503.924022	350003.432261	45.801204
3503.783250	350008.035700	45.806209
3503.560486	349998.297656	45.811213
3503.447905	350009.946606	45.816218
3503.584651	350003.485828	45.821223
3504.074438	350000.023376	45.826228
3503.652244	349987.593585	45.831233
3503.829339	349967.866373	45.836237
3503.817994	349973.518303	45.841242
3503.507169	349974.381857	45.846247
3503.864996	349978.117490	45.851252
3503.828920	349976.519750	45.856257
3503.809042	349964.866241	45.861261
3503.539116	349972.416984	45.866266
3503.516381	349985.247939	45.871271
3503.912006	349969.507463	45.876276
3503.729069	349980.047690	45.881281
3503.974189	349969.370335	45.886285
3503.653642	349951.579723	45.891290
3503.512060	349953.001899	45.896295
3503.947551	349949.293515	45.901300
3503.752747	349943.801386	45.906305
3503.786858	349941.047246	45.911309
3503.782077	349960.060004	45.916314
3503.591855	349945.735597	45.921319
3503.894206	349949.123686	45.926324
3503.925415	349957.695774	45.931329
3504.373398	349933.802638	45.936333
3504.199949	349923.038737	45.941338
3504.083946	349926.645671	45.946343
3504.018372	349916.831861	45.951348
3503.899162	349892.544800	45.956353
3503.905246	349878.087537	45.961357
3503.457396	349885.004688	45.966362
3503.530627	349876.517841	45.971367
3503.881760	349874.018995	45.976372
3503.620909	349879.786731	45.981377
3503.655109	349881.308376	45.986381
3503.748922	349873.759969	45.991386
3503.613105	349883.452875	45.996391
3503.596006	349883.964581	46.001396
3503.441141	349887.246796	46.006401
3504.023596	349875.650754	46.011405
3503.848585	349879.852397	46.016410
3503.798021	349863.673404	46.021415
3503.815028	349849.672528	46.026420
3503.846040	349850.354788	46.031425
3503.481057	349845.093162	46.036429
3503.755799	349858.818814	46.041434
3503.648821	349855.679755	46.046439
3503.943496	349848.023237	46.051444
3503.942465	349858.203864	46.056449
3503.677180	349853.053734	46.061453
3503.704694	349839.509317	46.066458
3503.469554	349837.815786	46.071463
3503.723388	349817.083791	46.076468
3503.122947	349832.856647	46.081473
3503.153443	349826.132682	46.086477
3503.780768	349844.180210	46.091482
3503.705216	349849.485986	46.096487
3503.811120	349831.806077	46.101492
3503.464170	349828.195929	46.106497
3503.532562	349829.559462	46.111501
3503.795113	349833.411972	46.116506
3503.551725	349831.617940	46.121511
3503.746945	349827.260349	46.126516
3503.693482	349834.369671	46.131521
3503.962443	349822.212348	46.136525
3504.004462	349833.302419	46.141530
3503.639780	349842.700647	46.146535
3503.925064	349839.194161	46.151540
3503.845406	349821.747193	46.156545
3503.921249	349805.522748	46.161549
3503.691979	349808.791279	46.166554
3503.531096	349809.223911	46.171559
3504.076482	349795.215845	46.176564
3503.958068	349806.254930	46.181569
3503.697284	349806.881514	46.186573
3503.600037	349806.006074	46.191578
3503.898193	349802.523001	46.196583
3503.999435	349790.646698	46.201588
3503.528018	349777.842872	46.206593
3503.650656	349779.528697	46.211597
3503.818638	349779.909340	46.216602
3503.556687	349778.525461	46.221607
3503.546359	349776.338265	46.226612
3503.777976	349785.489529	46.231617
3503.744025	349776.892354	46.236621
3503.567044	349787.228066	46.241626
3503.729557	349784.555424	46.246631
3503.953956	349781.338523	46.251636
3503.733547	349782.518652	46.256641
3503.907418	349750.040797	46.261645
3503.946515	349740.363115	46.266650
3503.658492	349758.326315	46.271655
3503.966266	349746.570059	46.276660
3503.648691	349757.029808	46.281665
3503.799269	349748.505262	46.286669
3504.031408	349749.308435	46.291674
3503.657476	349741.859405	46.296679
3503.866282	349720.065539	46.301684
3503.601341	349720.692782	46.306689
3503.856859	349716.936480	46.311693
3503.857189	349717.496336	46.316698
3503.723030	349730.344965	46.321703
3503.707012	349726.071663	46.326708
3503.868727	349718.308890	46.331713
3503.967911	349720.889219	46.336717
3503.630700	349708.191417	46.341722
3503.762503	349692.212605	46.346727
3503.905833	349695.931265	46.351732
3503.559181	349689.979541	46.356737
3503.779943	349688.493897	46.361741
3503.877325	349689.394728	46.366746
3503.685154	349688.101620	46.371751
3503.884931	349691.327782	46.376756
3503.834722	349696.655017	46.381761
3503.791104	349693.887701	46.386765
3503.780663	349671.084974	46.391770
3503.473118	349668.868406	46.396775
3503.804312	349653.748857	46.401780
3503.582941	349667.094863	46.406785
3503.466435	349668.945754	46.411789
3503.424492	349661.749646	46.416794
3503.637979	349671.285564	46.421799
3503.815280	349660.695225	46.426804
3503.698588	349670.385145	46.431809
3503.721226	349659.819256	46.436813
3503.757417	349657.064773	46.441818
3503.650477	349658.277869	46.446823
3503.876210	349664.375927	46.451828
3503.417480	349672.032912	46.456833
3503.624584	349671.083904	46.461837
3503.831260	349674.563489	46.466842
3503.557593	349674.555829	46.471847
3503.736615	349667.655657	46.476852
3503.607275	349656.197546	46.481857
3503.879494	349649.180833	46.486861
3503.700020	349644.398887	46.491866
3503.509198	349637.913497	46.496871
3503.914010	349638.485764	46.501876
3503.356039	349654.786434	46.506881
3503.904519	349635.458516	46.511885
3503.718026	349643.199725	46.516890
3503.734600	349641.822713	46.521895
3503.947504	349649.093560	46.526900
3503.927159	349657.673846	46.531905
3503.727993	349632.966638	46.536909
3503.610711	349613.947571	46.541914
3503.459420	349604.885344	46.546919
3503.950768	349609.134373	46.551924
3503.527003	349615.462370	46.556929
3503.647340	349610.556671	46.561933
3503.553654	349609.324346	46.566938
3503.545249	349623.120270	46.571943
3503.584580	349610.566530	46.576948
3503.525599	349619.738309	46.581953
3504.065643	349611.304881	46.586957
3503.893554	349618.636594	46.591962
3503.790461	349619.060092	46.596967
3503.784634	349612.570905	46.601972
3503.381230	349605.686446	46.606977
3503.692480	349601.259592	46.611981
3503.709105	349589.727489	46.616986
3503.313313	349605.951633	46.621991
3503.573262	349588.552710	46.626996
3503.720496	349597.691893	46.632001
3503.574690	349594.177187	46.637005
3503.824256	349595.028509	46.642010
3503.358374	349602.813892	46.647015
3503.838270	349596.069757	46.652020
3503.551563	349608.891628	46.657025
3503.392595	349601.383145	46.662029
3503.511319	349601.440709	46.667034
3503.249298	349600.794925	46.672039
3503.773171	349603.002706	46.677044
3503.316843	349617.098505	46.682049
3503.712622	349603.012236	46.687053
3503.673891	349605.436214	46.692058
3503.594484	349605.245136	46.697063
3503.646657	349614.806565	46.702068
3503.827451	349609.000512	46.707073
3503.454746	349612.291730	46.712077
3504.032353	349614.338308	46.717082
3503.551063	349620.904460	46.722087
3504.017428	349618.285580	46.727092
3503.851039	349611.312750	46.732097
3503.847356	349585.200246	46.737101
3503.876445	349579.978102	46.742106
3503.490489	349580.039096	46.747111
3503.827734	349572.757580	46.752116
3503.450316	349581.928804	46.757121
3503.644125	349572.150281	46.762125
3504.029208	349576.161598	46.767130
3503.602231	349572.869500	46.772135
3504.000273	349581.180044	46.777140
3503.551933	349566.794538	46.782145
3503.589119	349546.783878	46.787149
3503.614877	349554.796961	46.792154
3503.499698	349554.636989	46.797159
3503.384422	349556.513140	46.802164
3503.988323	349550.843804	46.807169
3503.552758	349551.116252	46.812173
3503.756398	349548.488000	46.817178
3503.892198	349549.128246	46.822183
3504.104556	349548.407467	46.827188
3503.829221	349559.115090	46.832193
3503.999643	349547.609568	46.837197
3503.722377	349533.527876	46.842202
3503.598980	349518.734668	46.847207
3503.982849	349505.057479	46.852212
3503.705708	349519.761260	46.857217
3503.709465	349522.687553	46.862221
3503.883154	349507.491058	46.867226
3503.898622	349524.795522	46.872231
3503.655872	349522.034227	46.877236
3503.864257	349528.593166	46.882241
3503.727573	349508.737235	46.887245
3503.885224	349489.496503	46.892250
3503.376704	349491.969302	46.897255
3503.826788	349481.895735	46.902260
3503.601810	349492.519056	46.907265
3503.723713	349487.129522	46.912269
3503.510347	349497.165624	46.917274
3503.584078	349491.071068	46.922279
3504.102619	349490.021919	46.927284
3504.078296	349503.998550	46.932289
3503.914112	349498.094314	46.937293
3503.892850	349464.603632	46.942298
3503.799285	349470.115903	46.947303
3503.979907	349460.161285	46.952308
3503.958887	349455.277919	46.957313
3504.066125	349467.070392	46.962317
3503.726314	349462.721000	46.967322
3503.656424	349446.850357	46.972327
3503.862508	349439.258690	46.977332
3503.380169	349431.037763	46.982337
3503.725944	349421.540606	46.987341
3503.834173	349424.272228	46.992346
3503.468086	349427.613313	46.997351
3503.771978	349426.776256	47.002356
3503.689911	349438.802273	47.007361
3503.633257	349435.629783	47.012365
3503.699260	349426.125953	47.017370
3503.747377	349435.535346	47.022375
3503.741954	349420.876171	47.027380
3503.330989	349443.083843	47.032385
3503.584609	349429.605386	47.037389
3503.672109	349436.030738	47.042394
3503.453972	349443.217047	47.047399
3503.611228	349435.913064	47.052404
3503.462485	349441.255901	47.057409
3503.627502	349434.790588	47.062413
3503.739317	349438.386990	47.067418
3503.369792	349426.152357	47.072423
3503.928892	349410.258621	47.077428
3503.691837	349411.466841	47.082433
3503.615386	349406.795845	47.087437
3503.827904	349402.053715	47.092442
3503.728926	349411.359109	47.097447
3503.956916	349400.811610	47.102452
3503.715782	349407.568884	47.107457
3503.397058	349405.914004	47.112461
3503.455631	349413.336538	47.117466
3503.560101	349426.172965	47.122471
3503.458286	349401.984744	47.127476
3503.574486	349411.536087	47.132481
3503.592996	349416.674325	47.137485
3503.632478	349419.009593	47.142490
3503.357413	349414.191836	47.147495
3503.759041	349410.768736	47.152500
3503.507993	349423.101436	47.157505
3503.812506	349411.243819	47.162509
3503.667389	349399.126412	47.167514
3503.612877	349396.488061	47.172519
3504.107359	349389.690692	47.177524
3503.693837	349388.687084	47.182529
3503.640534	349394.294804	47.187533
3503.902905	349385.192597	47.192538
3503.824879	349387.317380	47.197543
3503.623377	349388.825397	47.202548
3503.741400	349391.835438	47.207553
3503.658814	349387.012701	47.212557
3503.571296	349398.479657	47.217562
3503.192182	349410.221772	47.222567
3503.796260	349397.985926	47.227572
3503.605433	349394.656485	47.232577
3503.514578	349392.914678	47.237581
3503.575295	349365.595673	47.242586
3503.809264	349358.584970	47.247591
3503.956445	349365.917148	47.252596
3503.541462	349362.088660	47.257601
3503.684725	349358.350081	47.262605
3504.094374	349369.229418	47.267610
3503.825112	349359.396806	47.272615
3503.833019	349353.516252	47.277620
3503.627871	349365.587194	47.282625
3503.578986	349369.539874	47.287629
3503.652897	349356.242518	47.292634
3503.485799	349345.935626	47.297639
3503.712638	349333.352180	47.302644
3503.739912	349338.438138	47.307649
3503.853404	349327.526954	47.312653
3503.703205	349319.329857	47.317658
3503.574263	349333.094006	47.322663
3503.578654	349325.610563	47.327668
3503.669119	349333.842512	47.332673
3503.440215	349334.667673	47.337677
3503.731920	349328.360480	47.342682
3503.621243	349328.937888	47.347687
3504.021662	349322.308090	47.352692
3503.731628	349340.169937	47.357697
3503.643310	349327.025477	47.362701
3503.722436	349334.801093	47.367706
3503.402529	349321.082408	47.372711
3503.682526	349297.241004	47.377716
3503.517031	349298.361559	47.382721
3503.527562	349295.432954	47.387725
3503.505530	349287.673718	47.392730
3503.564972	349296.928635	47.397735
3503.717221	349299.729659	47.402740
3503.780730	349297.785286	47.407745
3503.611716	349300.458937	47.412749
3503.875607	349300.391747	47.417754
3503.222530	349306.476064	47.422759
3503.704558	349309.097696	47.427764
3503.812935	349304.677438	47.432769
3503.905814	349309.880285	47.437773
3503.852394	349313.146496	47.442778
3503.639213	349317.863245	47.447783
3503.805434	349315.240898	47.452788
3503.413583	349314.157508	47.457793
3503.616199	349305.522862	47.462797
3504.030809	349295.658481	47.467802
3503.759124	349285.088146	47.472807
3503.801068	349272.355755	47.477812
3503.622218	349286.153258	47.482817
3503.484522	349273.500169	47.487821
3503.749798	349282.671647	47.492826
3503.704353	349274.483434	47.497831
3503.842563	349272.730863	47.502836
3503.420827	349289.213716	47.507841
3503.650969	349292.409650	47.512845
3503.719035	349280.411224	47.517850
3503.602317	349298.958327	47.522855
3503.932659	349287.020246	47.527860
3503.541493	349272.931042	47.532865
3503.653847	349258.075045	47.537869
3503.965651	349262.886965	47.542874
3503.458097	349260.116616	47.547879
3503.614592	349259.633728	47.552884
3503.168958	349258.787903	47.557889
3503.502931	349253.313918	47.562893
3503.791825	349256.933241	47.567898
3503.835793	349260.031351	47.572903
3503.872638	349253.764439	47.577908
3503.532937	349260.588217	47.582913
3503.779962	349258.360316	47.587917
3503.931506	349257.191021	47.592922
3503.744131	349265.008777	47.597927
3504.117753	349261.819158	47.602932
3503.721120	349239.637237	47.607937
3503.654656	349228.652676	47.612941
3503.531871	349231.828052	47.617946
3503.224680	349234.116326	47.622951
3503.899208	349231.031846	47.627956
3503.643531	349239.038563	47.632961
3504.013101	349232.540889	47.637965
3503.707366	349230.731241	47.642970
3503.708686	349244.907495	47.647975
3504.005755	349222.285032	47.652980
3503.707948	349223.579215	47.657985
3503.585606	349210.338300	47.662989
3503.732161	349191.531893	47.667994
3503.472907	349207.480054	47.672999
3503.551522	349187.055490	47.678004
3503.344435	349198.286874	47.683009
3503.272830	349200.130682	47.688013
3503.687859	349192.149629	47.693018
3502.881697	349201.541404	47.698023
3503.552069	349210.419789	47.703028
3503.533168	349242.008070	47.708033
3503.742884	349233.321387	47.713037
3503.920508	349226.650444	47.718042
3503.801230	349215.063394	47.723047
3503.590066	349201.607455	47.728052
3503.874989	349202.427743	47.733057
3504.072316	349208.733953	47.738061
3504.088273	349197.583647	47.743066
3503.659465	349207.144830	47.748071
3503.689986	349199.122758	47.753076
3504.021276	349197.085146	47.758081
3503.927645	349182.541658	47.763085
3503.978349	349180.472048	47.768090
3503.823231	349184.136117	47.773095
3503.875010	349185.476841	47.778100
3503.565748	349183.973168	47.783105
3503.697037	349180.109212	47.788109
3503.843932	349190.393835	47.793114
3503.665046	349177.161851	47.798119
3503.924814	349146.807990	47.803124
3503.511225	349155.985003	47.808129
3503.674923	349147.738257	47.813133
3504.041889	349142.666270	47.818138
3503.721039	349150.530594	47.823143
3503.558065	349142.793618	47.828148
3503.680337	349151.962273	47.833153
3503.797935	349156.244970	47.838157
3504.252639	349151.769951	47.843162
3503.553039	349141.419946	47.848167
3503.365456	349123.099016	47.853172
3503.484571	349116.895437	47.858177
3503.359842	349124.906921	47.863181
3503.523115	349115.413112	47.868186
3503.654219	349119.388259	47.873191
3503.750694	349114.104515	47.878196
3503.500629	349113.609544	47.883201
3503.460895	349116.924506	47.888205
3503.550277	349115.459617	47.893210
3503.109778	349125.099016	47.898215
3503.289627	349121.354637	47.903220
3503.535399	349142.440546	47.908225
3503.143136	349155.839142	47.913229
3503.795826	349165.687488	47.918234
3503.628752	349174.240141	47.923239
3503.572250	349148.161233	47.928244
3503.488191	349137.383047	47.933249
3503.714512	349132.511455	47.938253
3503.273993	349125.174674	47.943258
3503.160551	349151.356773	47.948263
3503.577654	349146.531375	47.953268
3503.019076	349166.904531	47.958273
3503.196786	349174.588230	47.963277
3503.909665	349173.864675	47.968282
3503.814320	349174.516015	47.973287
3503.892804	349176.336096	47.978292
3503.850661	349154.327165	47.983297
3503.717159	349148.545298	47.988301
3504.069582	349137.163628	47.993306
3503.779410	349140.747244	47.998311
3503.870975	349151.091525	48.003316
3503.733152	349149.967973	48.008321
3503.484779	349152.577822	48.013325
3503.825849	349142.648685	48.018330
3503.567082	349150.299582	48.023335
3503.637403	349141.813082	48.028340
3503.574643	349123.955998	48.033345
3503.575776	349118.890940	48.038349
3503.829630	349105.056045	48.043354
3503.615353	349114.583329	48.048359
3503.694837	349101.030515	48.053364
3503.690622	349112.255297	48.058369
3503.625385	349101.932257	48.063373
3503.724455	349109.093914	48.068378
3503.907508	349108.683181	48.073383
3504.142876	349101.443161	48.078388
3503.908701	349114.664066	48.083393
3503.685249	349098.410374	48.088397
3503.857204	349083.952132	48.093402
3503.231123	349079.367998	48.098407
3503.675783	349069.320666	48.103412
3503.485772	349071.055939	48.108417
3503.322772	349079.735221	48.113421
3503.396662	349079.698067	48.118426
3503.307932	349075.996144	48.123431
3503.852743	349083.010983	48.128436
3503.910506	349082.212832	48.133441
3503.831637	349078.687511	48.138445
3504.068255	349083.409527	48.143450
3503.784563	349087.882927	48.148455
3503.655589	349084.060109	48.153460
3503.825829	349082.277017	48.158465
3503.450154	349094.476782	48.163469
3503.924095	349085.417435	48.168474
3503.414170	349071.754180	48.173479
3503.520380	349055.499262	48.178484
3503.531889	349055.497422	48.183489
3503.562838	349058.164924	48.188493
3503.824394	349046.517633	48.193498
3503.584786	349054.114612	48.198503
3503.760031	349059.864395	48.203508
3503.627794	349054.056868	48.208513
3503.776087	349048.993990	48.213517
3503.922318	349053.984814	48.218522
3503.772421	349055.408327	48.223527
3503.754630	349050.040835	48.228532
3503.634112	349064.898137	48.233537
3503.589990	349057.855004	48.238541
3503.994479	349051.988078	48.243546
3503.574772	349048.389380	48.248551
3503.632662	349033.541932	48.253556
3503.439010	349027.565950	48.258561
3503.636148	349029.749052	48.263565
3503.715661	349036.939262	48.268570
3503.614899	349036.980622	48.273575
3503.793206	349032.422029	48.278580
3503.602585	349043.269068	48.283585
3503.510126	349037.658863	48.288589
3503.946309	349029.750798	48.293594
3503.785484	349041.433029	48.298599
3503.786970	349020.715178	48.303604
3503.884077	349042.817238	48.308609
3503.820882	349015.543101	48.313613
3503.812016	348998.542811	48.318618
3503.893401	349001.635020	48.323623
3503.780813	348994.399090	48.328628
3503.690302	349005.993859	48.333633
3503.489250	349004.931203	48.338637
3503.887531	348997.130930	48.343642
3503.472347	349001.166996	48.348647
3503.465144	348994.245276	48.353652
3503.705818	349001.639077	48.358657
3503.677461	349004.723183	48.363661
3503.569182	348999.777217	48.368666
3503.456261	349010.052044	48.373671
3503.896551	348999.699971	48.378676
3503.435303	348988.497805	48.383681
3503.591668	348982.542839	48.388685
3503.596535	348963.631497	48.393690
3503.610803	348968.897706	48.398695
3503.791269	348967.367510	48.403700
3503.799628	348970.878491	48.408705
3503.500122	348967.820721	48.413709
3503.555063	348968.779176	48.418714
3503.706690	348977.561444	48.423719
3503.680924	348973.569593	48.428724
3503.633089	348974.671554	48.433729
3503.555151	348983.591919	48.438733
3503.803801	348979.531235	48.443738
3503.473755	348979.914261	48.448743
3503.556843	348967.200748	48.453748
3503.621626	348980.959810	48.458753
3503.559778	348973.690405	48.463757
3504.199665	348968.295289	48.468762
3503.442154	348963.808278	48.473767
3503.604059	348937.491130	48.478772
3503.497279	348942.241993	48.483777
3503.539931	348953.001269	48.488781
3503.732312	348932.787691	48.493786
3503.703879	348942.285625	48.498791
3503.704516	348936.711596	48.503796
3503.443226	348936.218397	48.508801
3503.429835	348944.339564	48.513805
3503.779909	348935.885162	48.518810
3503.550295	348958.573391	48.523815
3503.803880	348947.665436	48.528820
3503.797659	348945.553914	48.533825
3503.365996	348944.324100	48.538829
3503.711656	348949.487019	48.543834
3503.392509	348944.065351	48.548839
3503.694073	348942.974139	48.553844
3503.330388	348957.793557	48.558849
3503.503740	348950.665127	48.563853
3503.782287	348952.326331	48.568858
3503.723932	348949.841276	48.573863
3503.756389	348953.373900	48.578868
3503.645925	348954.256697	48.583873
3503.695179	348967.610992	48.588877
3503.639182	348938.248646	48.593882
3503.545065	348929.482690	48.598887
3503.612823	348918.578655	48.603892
3503.436356	348919.319177	48.608897
3503.472630	348918.957099	48.613901
3503.855141	348919.303834	48.618906
3503.711913	348920.700845	48.623911
3503.689132	348920.373554	48.628916
3503.625331	348916.693131	48.633921
3503.514641	348914.139993	48.638925
3503.964429	348925.929331	48.643930
3503.825153	348923.228002	48.648935
3503.910352	348925.581515	48.653940
3503.696814	348936.508553	48.658945
3503.544473	348927.777252	48.663949
3503.704395	348924.621398	48.668954
3503.597956	348915.628322	48.673959
3503.479779	348898.594380	48.678964
3503.581647	348890.179209	48.683969
3503.686839	348901.921222	48.688973
3503.667389	348895.917686	48.693978
3503.469546	348900.072110	48.698983
3503.609289	348890.327465	48.703988
3503.716342	348892.321202	48.708993
3503.470704	348893.938016	48.713997
3504.015348	348891.128566	48.719002
3503.712955	348896.852069	48.724007
3503.916259	348889.693445	48.729012
3503.831686	348893.549994	48.734017
3503.670496	348895.077103	48.739021
3503.893437	348893.438383	48.744026
3503.422119	348888.677058	48.749031
3503.641701	348864.412341	48.754036
3503.326022	348857.513920	48.759041
3502.979905	348876.581010	48.764045
3503.668810	348884.463903	48.769050
3503.593030	348901.452116	48.774055
3503.811460	348900.348595	48.779060
3503.622563	348889.688742	48.784065
3503.556074	348882.521864	48.789069
3503.736960	348870.276450	48.794074
3503.587454	348872.997940	48.799079
3503.691837	348866.440340	48.804084
3503.616100	348869.506492	48.809089
3503.614607	348866.528862	48.814093
3503.822878	348867.590338	48.819098
3503.571100	348867.171990	48.824103
3503.494565	348870.187365	48.829108
3503.691804	348877.257177	48.834113
3503.837380	348868.122447	48.839117
3503.721924	348872.162041	48.844122
3503.784663	348873.271975	48.849127
3504.304224	348876.345824	48.854132
3503.891196	348848.770586	48.859137
3503.770880	348853.243629	48.864141
3503.972958	348845.423449	48.869146
3503.767319	348848.790107	48.874151
3503.691243	348840.403059	48.879156
3503.677546	348847.098995	48.884161
3503.711237	348842.461443	48.889165
3503.786042	348842.296886	48.894170
3503.559026	348827.036293	48.899175
3503.951407	348806.129308	48.904180
3503.767985	348804.809344	48.909185
3503.721413	348815.964527	48.914189
3504.004177	348808.716976	48.919194
3503.394524	348817.034230	48.924199
3503.544355	348803.342964	48.929204
3503.710538	348814.006383	48.934209
3503.653820	348817.858533	48.939213
3503.780356	348803.560109	48.944218
3503.459242	348821.274326	48.949223
3503.305786	348802.896992	48.954228
3503.431871	348811.327001	48.959233
3503.295253	348816.566175	48.964237
3503.807850	348803.733820	48.969242
3503.770530	348816.618256	48.974247
3503.617525	348815.191677	48.979252
3503.102318	348815.833041	48.984257
3503.401315	348820.519766	48.989261
3503.573537	348818.252771	48.994266
3503.371419	348825.105754	48.999271
3503.588497	348817.232296	49.004276
3503.551358	348822.913873	49.009281
3503.475436	348823.740309	49.014285
3503.876073	348814.259827	49.019290
3503.807001	348815.416052	49.024295
3503.749536	348814.101628	49.029300
3503.719929	348797.664493	49.034305
3503.658265	348782.555909	49.039309
3503.883847	348788.883153	49.044314
3503.818399	348787.697248	49.049319
3503.653267	348779.451529	49.054324
3503.452231	348793.481726	49.059329
3503.634872	348789.915045	49.064333
3503.566838	348777.530800	49.069338
3503.946850	348791.112817	49.074343
3503.722684	348787.279576	49.079348
3503.605501	348793.304681	49.084353
3503.482788	348790.702535	49.089357
3503.724602	348781.883448	49.094362
3503.297953	348794.473113	49.099367
3503.439120	348788.240560	49.104372
3503.722362	348789.086572	49.109377
3503.652718	348796.147682	49.114381
3503.863367	348789.827790	49.119386
3503.992960	348780.975541	49.124391
3503.766698	348769.608924	49.129396
3503.642960	348771.079212	49.134401
3503.705209	348760.965021	49.139405
3503.561595	348767.986925	49.144410
3503.372042	348765.878926	49.149415
3503.644062	348766.090419	49.154420
3503.746475	348765.666981	49.159425
3503.323203	348773.140322	49.164429
3503.448218	348769.964525	49.169434
3503.575407	348782.390283	49.174439
3503.904933	348772.946488	49.179444
3503.665644	348777.540151	49.184449
3503.670732	348772.779857	49.189453
3504.026152	348770.712963	49.194458
3503.439128	348759.861507	49.199463
3503.477620	348738.501408	49.204468
3503.874607	348735.180807	49.209473
3503.630371	348743.491208	49.214477
3503.633842	348744.330545	49.219482
3503.398955	348747.294605	49.224487
3503.797478	348742.904789	49.229492
3503.622010	348745.910359	49.234497
3503.238942	348744.749214	49.239501
3503.907224	348742.938281	49.244506
3503.491944	348746.490797	49.249511
3503.902022	348740.342986	49.254516
3503.876616	348747.142591	49.259521
3503.719194	348744.851350	49.264525
3503.803099	348744.125417	49.269530
3503.534870	348754.144874	49.274535
3504.103028	348744.052508	49.279540
3503.745389	348720.108046	49.284545
3503.732306	348706.976997	49.289549
3503.757170	348699.337524	49.294554
3503.634733	348712.693570	49.299559
3503.316981	348707.678886	49.304564
3503.751116	348709.799083	49.309569
3503.666157	348711.721374	49.314573
3503.612775	348704.221529	49.319578
3503.504315	348719.077017	49.324583
3503.466064	348709.436835	49.329588
3503.752194	348713.463859	49.334593
3503.565325	348707.919449	49.339597
3503.889206	348704.508597	49.344602
3503.703578	348717.238338	49.349607
3503.839812	348700.215019	49.354612
3503.727040	348688.219603	49.359617
3503.510996	348680.898180	49.364621
3503.800096	348673.496899	49.369626
3503.517640	348674.839571	49.374631
3503.855679	348663.205561	49.379636
3503.793057	348667.185914	49.384641
3503.763204	348682.614375	49.389645
3503.889660	348670.326618	49.394650
3503.486890	348678.229411	49.399655
3503.775469	348674.136940	49.404660
3503.781380	348680.727989	49.409665
3503.868163	348669.973609	49.414669
3503.810725	348654.762516	49.419674
3503.465544	348655.402454	49.424679
3503.732980	348637.365756	49.429684
3503.275431	348645.124502	49.434689
3503.343404	348637.045525	49.439693
3503.616016	348645.808719	49.444698
3503.462793	348639.673593	49.449703
3503.291483	348647.717961	49.454708
3503.470398	348654.205308	49.459713
3503.734054	348639.376130	49.464717
3503.782195	348644.967887	49.469722
3503.379883	348661.626017	49.474727
3503.630294	348642.930266	49.479732
3503.537729	348653.227392	49.484737
3503.549359	348654.930801	49.489741
3503.887671	348642.253221	49.494746
3503.590461	348656.502271	49.499751
3503.539490	348644.089846	49.504756
3503.625956	348650.820874	49.509761
3503.367140	348648.469303	49.514765
3503.736376	348646.883805	49.519770
3503.414461	348652.584967	49.524775
3503.598395	348649.578011	49.529780
3503.796411	348657.360378	49.534785
3503.612695	348652.706276	49.539789
3503.629121	348661.000933	49.544794
3503.421451	348669.967309	49.549799
3503.522112	348665.268252	49.554804
3503.587489	348672.460743	49.559809
3503.824342	348676.826432	49.564813
3503.909084	348662.865452	49.569818
3503.726204	348660.094648	49.574823
3503.734607	348637.084903	49.579828
3503.460328	348629.187289	49.584833
3503.123370	348638.784952	49.589837
3503.945209	348637.993262	49.594842
3503.796001	348638.373154	49.599847
3503.605398	348631.556738	49.604852
3503.801095	348637.812368	49.609857
3503.616388	348639.699526	49.614861
3504.153124	348640.683628	49.619866
3503.843782	348636.151192	49.624871
3503.784269	348627.863301	49.629876
3503.801663	348603.197755	49.634881
3503.143566	348611.853571	49.639885
3503.254567	348602.826070	49.644890
3503.253547	348626.216397	49.649895
3503.837006	348625.691459	49.654900
3503.550792	348624.540451	49.659905
3503.555472	348623.547071	49.664909
3503.804870	348619.613501	49.669914
3503.853566	348619.325813	49.674919
3503.892806	348603.132254	49.679924
3503.756810	348607.429633	49.684929
3503.816841	348605.714852	49.689933
3504.066990	348601.272127	49.694938
3503.962738	348605.971716	49.699943
3503.740207	348588.954175	49.704948
3503.499659	348575.299116	49.709953
3503.719928	348572.668190	49.714957
3503.769583	348563.370411	49.719962
3503.667837	348576.239635	49.724967
3503.863972	348571.754542	49.729972
3503.712686	348562.055849	49.734977
3503.794738	348579.884570	49.739981
3503.847676	348569.390038	49.744986
3503.696722	348559.818551	49.749991
3503.901208	348569.763311	49.754996
3503.929627	348545.401418	49.760001
3503.878634	348536.170449	49.765005
3504.076512	348527.154654	49.770010
3503.598730	348536.596434	49.775015
3503.810403	348523.684330	49.780020
3503.956680	348536.794323	49.785025
3503.765711	348534.941058	49.790029
3503.644134	348499.124086	49.795034
3503.469918	348498.973444	49.800039
3503.685967	348490.769229	49.805044
3503.399883	348497.610075	49.810049
3503.016034	348501.412155	49.815053
3503.563636	348508.604789	49.820058
3503.184673	348532.716651	49.825063
3503.812037	348544.401642	49.830068
3504.104091	348528.117192	49.835073
3503.688733	348503.443659	49.840077
3503.792200	348502.052882	49.845082
3503.747867	348504.146920	49.850087
3503.760528	348488.542923	49.855092
3503.929041	348503.863719	49.860097
3503.939367	348491.797896	49.865101
3504.042557	348482.008056	49.870106
3503.770899	348475.178983	49.875111
3503.814590	348464.838605	49.880116
3503.459482	348460.364293	49.885121
3503.510710	348471.987669	49.890125
3503.464161	348457.283837	49.895130
3503.439801	348464.388734	49.900135
3503.732458	348464.826033	49.905140
3503.554299	348459.941970	49.910145
3503.521141	348467.150064	49.915149
3503.851682	348457.426085	49.920154
3503.690140	348459.487751	49.925159
3503.720509	348464.293329	49.930164
3503.937222	348458.863256	49.935169
3503.895144	348461.949561	49.940173
3503.736252	348453.066510	49.945178
3503.397154	348439.452449	49.950183
3503.767633	348433.463576	49.955188
3503.471290	348432.543232	49.960193
3503.453860	348425.368541	49.965197
3503.680445	348428.285116	49.970202
3503.517853	348433.197557	49.975207
3503.557130	348431.435149	49.980212
3503.754469	348430.793086	49.985217
3503.532974	348440.550692	49.990221
3503.352547	348434.063518	49.995226
3503.187527	348443.914003	50.000231
3503.546340	348431.665817	50.005236
3503.641508	348435.290367	50.010241
3503.394685	348442.481339	50.015245
3503.707769	348439.683023	50.020250
3503.789154	348442.775263	50.025255
3503.649374	348438.317812	50.030260
3503.696496	348439.786550	50.035265
3503.823896	348430.476458	50.040269
3503.814550	348438.138926	50.045274
3503.579494	348443.877281	50.050279
3503.683276	348437.599696	50.055284
3503.729347	348451.998144	50.060289
3503.704282	348450.093196	50.065293
3503.967946	348433.991370	50.070298
3503.615137	348416.587143	50.075303
3503.857387	348409.625916	50.080308
3504.021546	348406.978400	50.085313
3503.785251	348411.444361	50.090317
3504.044111	348400.102784	50.095322
3503.767110	348406.407715	50.100327
3503.842529	348393.975255	50.105332
3503.644951	348380.720585	50.110337
3503.558997	348377.221792	50.115341
3503.842134	348371.297624	50.120346
3503.424730	348374.290557	50.125351
3503.567882	348379.536446	50.130356
3503.754806	348377.038042	50.135361
3503.719805	348378.850638	50.140365
3504.005773	348372.416985	50.145370
3503.690030	348385.141920	50.150375
3503.438350	348375.128191	50.155380
3503.516107	348376.159405	50.160385
3503.370175	348379.134873	50.165389
3503.428673	348372.813536	50.170394
3503.419621	348376.250951	50.175399
3503.663608	348385.553202	50.180404
3503.776617	348372.223978	50.185409
3503.879079	348381.803121	50.190413
3503.902357	348365.230239	50.195418
3503.743692	348359.783144	50.200423
3503.782151	348335.954062	50.205428
3503.785894	348348.348527	50.210433
3503.454090	348345.728511	50.215437
3503.786764	348350.409952	50.220442
3503.620506	348343.869624	50.225447
3503.759115	348344.662151	50.230452
3503.578360	348344.970677	50.235457
3503.619421	348352.472476	50.240461
3503.649051	348348.319111	50.245466
3503.591279	348368.257059	50.250471
3503.662545	348342.590257	50.255476
3503.944635	348351.479259	50.260481
3503.695546	348336.909223	50.265485
3503.529146	348321.766169	50.270490
3503.459147	348312.360005	50.275495
3503.604891	348310.529858	50.280500
3503.787410	348307.777628	50.285505
3503.451649	348312.412032	50.290509
3503.540254	348310.234591	50.295514
3503.623466	348313.708328	50.300519
3503.251304	348310.509296	50.305524
3503.510763	348303.927114	50.310529
3503.377244	348325.887753	50.315533
3503.544562	348308.375815	50.320538
3503.476111	348311.109971	50.325543
3503.567772	348316.898497	50.330548
3503.701804	348313.288567	50.335553
3503.596931	348311.370779	50.340557
3503.576456	348314.479129	50.345562
3503.637095	348313.731416	50.350567
3503.808788	348316.045829	50.355572
3503.674732	348311.103877	50.360577
3503.530055	348325.405253	50.365581
3503.614447	348321.421392	50.370586
3503.652103	348325.894955	50.375591
3503.688289	348318.737226	50.380596
3503.535675	348326.167838	50.385601
3503.688481	348330.012351	50.390605
3503.983533	348318.003287	50.395610
3503.635681	348325.210245	50.400615
3503.758157	348303.836703	50.405620
3504.079905	348293.579596	50.410625
3503.703265	348293.384598	50.415629
3503.959664	348287.031965	50.420634
3503.849461	348293.819579	50.425639
3503.583917	348295.363201	50.430644
3503.712875	348289.361591	50.435649
3503.643126	348297.211790	50.440653
3503.942293	348284.005827	50.445658
3503.564698	348275.182775	50.450663
3503.564499	348262.685884	50.455668
3503.689754	348255.997653	50.460673
3503.540928	348251.388905	50.465677
3503.133007	348258.910791	50.470682
3503.328309	348256.945548	50.475687
3503.670418	348273.155233	50.480692
3503.804207	348261.095295	50.485697
3503.410698	348266.935074	50.490701
3503.617811	348244.555504	50.495706
3503.240550	348262.940524	50.500711
3503.383849	348258.514663	50.505716
3503.910643	348261.332884	50.510721
3503.477158	348274.203717	50.515725
3503.408550	348255.761885	50.520730
3503.333535	348262.773008	50.525735
3503.564997	348242.553003	50.530740
3503.561869	348210.560366	50.535745
3503.120619	348183.549204	50.540749
3503.274828	348129.210260	50.545754
3503.068674	348080.451321	50.550759
3502.801776	348023.582740	50.555764
3502.896484	347946.651602	50.560769
3502.455909	347861.303972	50.565773
3502.226033	347774.166705	50.570778
3501.604290	347689.331048	50.575783
3501.551010	347587.199680	50.580788
3501.364288	347485.700079	50.585793
3500.936236	347373.828441	50.590797
3500.582076	347258.966972	50.595802
3500.137269	347139.105470	50.600807
3499.585928	347017.529788	50.605812
3499.112520	346883.062533	50.610817
3498.668576	346761.902022	50.615821
3498.201001	346633.720055	50.620826
3497.960568	346495.829856	50.625831
3497.311090	346354.796941	50.630836
3496.589741	346216.854838	50.635841
3495.843692	346067.844292	50.640845
3495.717817	345916.368191	50.645850
3495.147656	345777.993894	50.650855
3494.731731	345620.072347	50.655860
3494.000604	345469.887065	50.660865
3493.500272	345310.119941	50.665869
3493.492960	345142.129375	50.670874
3492.253225	344988.536160	50.675879
3491.953069	344822.754516	50.680884
3491.313957	344642.135673	50.685889
3490.984396	344487.531840	50.690893
3490.654403	344315.950069	50.695898
3489.995710	344142.968905	50.700903
3489.191083	343963.748667	50.705908
3488.470683	343787.289051	50.710913
3487.562611	343612.411277	50.715917
3487.245495	343432.043307	50.720922
3486.564421	343262.143076	50.725927
3486.078130	343089.971602	50.730932
3485.857715	342904.165022	50.735937
3484.746561	342726.542270	50.740941
3484.243084	342540.117513	50.745946
3483.837979	342351.385729	50.750951
3483.174538	342166.766938	50.755956
3482.183709	341979.424791	50.760961
3481.911449	341802.914009	50.765965
3481.332563	341609.854659	50.770970
3480.315158	341430.686043	50.775975
3480.003458	341235.852354	50.780980
3479.451671	341049.608908	50.785985
3478.343667	340861.009151	50.790989
3477.768324	340668.277235	50.795994
3477.301969	340478.556675	50.800999
3476.444158	340291.264780	50.806004
3476.054959	340106.189230	50.811009
3475.025383	339912.788610	50.816013
3474.717334	339721.895253	50.821018
3473.589405	339531.436415	50.826023
3472.895572	339344.472180	50.831028
3472.722797	339149.508263	50.836033
3471.644657	338974.949778	50.841037
3471.251012	338777.117682	50.846042
3470.415693	338585.413347	50.851047
3469.803408	338399.604455	50.856052
3469.332322	338217.107467	50.861057
3468.414046	338024.549084	50.866061
3467.899670	337828.311477	50.871066
3466.897820	337639.609080	50.876071
3466.028057	337440.320821	50.881076
3465.501908	337236.751845	50.886081
3464.957423	337069.155359	50.891085
3464.241372	336877.529003	50.896090
3463.584565	336689.965811	50.901095
3462.853313	336500.606428	50.906100
3462.374113	336321.007569	50.911105
3461.384600	336134.462789	50.916109
3461.002332	335940.235283	50.921114
3460.422975	335768.211531	50.926119
3459.327201	335581.503826	50.931124
3459.185591	335383.443558	50.936129
3458.521751	335200.917881	50.941133
3457.868205	335016.022553	50.946138
3457.237405	334831.301334	50.951143
3456.228164	334631.899542	50.956148
3455.414880	334444.125777	50.961153
3454.929743	334267.908320	50.966157
3454.425975	334070.181573	50.971162
3454.064990	333882.156576	50.976167
3453.349317	333695.103638	50.981172
3452.854103	333511.503084	50.986177
3451.780526	333327.789832	50.991181
3451.330485	333134.939897	50.996186
3450.732485	332944.022195	51.001191
3450.088967	332744.633590	51.006196
3449.499196	332550.073006	51.011201
3448.676502	332365.299272	51.016205
3447.911454	332172.522006	51.021210
3447.126447	331979.772838	51.026215
3446.307990	331802.456331	51.031220
3445.885415	331596.359474	51.036225
3444.867003	331406.598891	51.041229
3444.490432	331216.430828	51.046234
3443.965526	331023.739843	51.051239
3443.288802	330834.432933	51.056244
3442.406943	330641.160916	51.061249
3441.640780	330466.506105	51.066253
3441.344614	330254.631771	51.071258
3440.244176	330072.747591	51.076263
3439.457344	329882.844651	51.081268
3439.108050	329700.484374	51.086273
3438.314941	329508.773876	51.091277
3437.816423	329317.067232	51.096282
3436.861583	329124.897607	51.101287
3436.282214	328948.682174	51.106292
3435.575863	328751.456794	51.111297
3434.196403	328570.631515	51.116301
3434.209381	328387.090593	51.121306
3433.598930	328196.926431	51.126311
3432.575713	328009.576730	51.131316
3432.241830	327839.786750	51.136321
3431.452354	327640.127536	51.141325
3430.842461	327457.955911	51.146330
3430.110472	327269.412691	51.151335
3429.561773	327093.366426	51.156340
3429.030457	326911.130196	51.161345
3428.017988	326718.887369	51.166349
3427.403794	326534.448341	51.171354
3426.874060	326351.090330	51.176359
3426.085184	326168.205703	51.181364
3425.419784	325980.794633	51.186369
3424.838277	325787.768545	51.191373
3424.057619	325608.191227	51.196378
3423.002780	325429.853519	51.201383
3422.515584	325234.952583	51.206388
3422.267167	325060.356590	51.211393
3421.243550	324880.688795	51.216397
3420.792686	324693.699154	51.221402
3420.189942	324510.857781	51.226407
3419.538448	324322.575064	51.231412
3419.250942	324137.977143	51.236417
3418.300993	323949.333404	51.241421
3417.607999	323758.484415	51.246426
3416.442408	323579.982034	51.251431
3415.806604	323389.988855	51.256436
3415.496290	323205.978122	51.261441
3414.503987	323038.752041	51.266445
3414.122360	322848.870241	51.271450
3413.302814	322675.454470	51.276455
3412.200743	322493.298796	51.281460
3411.994419	322305.323164	51.286465
3411.272856	322133.902288	51.291469
3410.552319	321950.233838	51.296474
3409.860084	321775.930454	51.301479
3409.246675	321583.536383	51.306484
3408.849702	321399.942935	51.311489
3407.770017	321223.586401	51.316493
3407.396711	321038.129748	51.321498
3406.508987	320855.427569	51.326503
3405.914713	320682.532436	51.331508
3405.517760	320498.300593	51.336513
3404.780124	320315.420819	51.341517
3404.207649	320130.910442	51.346522
3403.130845	319964.099332	51.351527
3402.696854	319776.841884	51.356532
3402.212187	319584.550523	51.361537
3401.258192	319412.320975	51.366541
3400.500931	319229.009291	51.371546
3400.213574	319046.794217	51.376551
3399.236644	318859.620784	51.381556
3398.759614	318672.775331	51.386561
3397.969913	318501.511178	51.391565
3397.736040	318310.017820	51.396570
3396.747979	318132.189528	51.401575
3396.021068	317943.217827	51.406580
3395.422459	317760.616645	51.411585
3394.593580	317596.512135	51.416589
3394.267004	317408.927472	51.421594
3393.408084	317226.162747	51.426599
3392.608281	317044.457781	51.431604
3391.885044	316865.694091	51.436609
3391.183729	316688.963662	51.441613
3390.440947	316503.327364	51.446618
3389.793160	316322.284543	51.451623
3389.156385	316146.586941	51.456628
3388.580263	315963.953419	51.461633
3387.669366	315783.231333	51.466637
3387.276478	315608.054423	51.471642
3386.467277	315433.732414	51.476647
3386.013173	315255.661749	51.481652
3385.446460	315072.643193	51.486657
3384.413767	314896.522242	51.491661
3384.032595	314720.603528	51.496666
3383.408363	314545.461400	51.501671
3382.665859	314363.258771	51.506676
3382.335271	314184.963034	51.511681
3381.232589	314007.323834	51.516685
3380.762220	313823.727661	51.521690
3380.136308	313640.461336	51.526695
3379.195492	313459.867283	51.531700
3378.695503	313277.115169	51.536705
3377.964080	313110.263426	51.541709
3377.627770	312919.896553	51.546714
3376.766054	312735.265466	51.551719
3375.516958	312573.154699	51.556724
3375.177884	312382.583620	51.561729
3374.374697	312200.539731	51.566733
3374.132695	312025.867827	51.571738
3373.568533	311846.000952	51.576743
3372.616507	311669.887457	51.581748
3372.116978	311485.859100	51.586753
3371.328007	311322.578793	51.591757
3370.594302	311134.716311	51.596762
3369.980965	310953.251542	51.601767
3368.991836	310771.107445	51.606772
3368.431020	310591.874684	51.611777
3367.457406	310429.029748	51.616781
3367.008136	310243.132548	51.621786
3366.369414	310073.104055	51.626791
3365.628232	309898.507870	51.631796
3365.294446	309729.551110	51.636801
3364.300720	309554.434136	51.641805
3364.088861	309367.479432	51.646810
3363.443130	309197.399875	51.651815
3362.354945	309027.008079	51.656820
3361.970918	308841.072925	51.661825
3361.144178	308673.465900	51.666829
3360.788533	308489.206417	51.671834
3359.889344	308325.684783	51.676839
3359.091543	308136.274367	51.681844
3358.501772	307966.387987	51.686849
3357.306707	307804.491305	51.691853
3357.209011	307618.865562	51.696858
3356.444856	307460.923797	51.701863
3355.959047	307289.568554	51.706868
3355.409551	307097.061490	51.711873
3354.569672	306923.011504	51.716877
3353.987821	306735.500229	51.721882
3353.503267	306555.969436	51.726887
3352.658255	306385.943085	51.731892
3352.070568	306194.077373	51.736897
3351.051039	306024.256418	51.741901
3350.802488	305835.698005	51.746906
3350.183332	305672.026881	51.751911
3349.383387	305494.148876	51.756916
3348.754602	305318.026166	51.761921
3347.833888	305143.222683	51.766925
3347.274589	304967.521452	51.771930
3346.169562	304787.016886	51.776935
3345.750442	304613.457628	51.781940
3345.053784	304434.517834	51.786945
3344.212844	304272.255288	51.791949
3343.541180	304090.688127	51.796954
3343.165575	303921.042885	51.801959
3342.051802	303748.814800	51.806964
3341.821505	303578.560459	51.811969
3340.802649	303412.887182	51.816973
3340.481217	303241.067971	51.821978
3339.977227	303070.321541	51.826983
3339.136323	302899.882861	51.831988
3338.927959	302725.345769	51.836993
3337.654901	302552.963222	51.841997
3337.117804	302365.719174	51.847002
3336.424182	302198.617944	51.852007
3335.766881	302023.667192	51.857012
3335.060856	301850.837647	51.862017
3334.659749	301675.845984	51.867021
3333.957068	301501.105553	51.872026
3333.277445	301343.016262	51.877031
3332.356318	301160.848370	51.882036
3332.024803	300986.736262	51.887041
3330.780095	300811.138545	51.892045
3330.293228	300642.194851	51.897050
3329.903903	300475.171007	51.902055
3329.140402	300298.274240	51.907060
3328.805805	300120.672787	51.912065
3327.854656	299961.402705	51.917069
3327.669612	299779.880854	51.922074
3326.788120	299604.402677	51.927079
3326.174622	299425.443939	51.932084
3325.563900	299240.398046	51.937089
3324.621496	299060.370416	51.942093
3323.687235	298886.886255	51.947098
3323.092744	298704.944164	51.952103
3322.206156	298537.869736	51.957108
3321.876932	298368.516855	51.962113
3321.234159	298196.844992	51.967117
3320.401198	298022.758233	51.972122
3320.037415	297852.315261	51.977127
3318.984259	297678.517669	51.982132
3318.543756	297496.015203	51.987137
3317.436503	297341.937233	51.992141
3316.795458	297165.170753	51.997146
3316.393325	296993.103178	52.002151
3315.748184	296828.841315	52.007156
3315.287129	296659.889732	52.012161
3314.234780	296486.192789	52.017165
3313.339078	296319.194219	52.022170
3313.150389	296165.886837	52.027175
3312.305726	296008.990361	52.032180
3311.829347	295837.493788	52.037185
3311.176592	295671.602271	52.042189
3310.319492	295495.836213	52.047194
3309.747628	295321.858528	52.052199
3308.839200	295155.956099	52.057204
3308.153751	294981.766890	52.062209
3307.520146	294830.286118	52.067213
3307.653074	294660.755045	52.072218
3306.497821	294492.140673	52.077223
3305.758541	294319.665747	52.082228
3304.852287	294139.194888	52.087233
3304.113065	293985.514574	52.092237
3303.503735	293818.672452	52.097242
3303.283593	293648.279616	52.102247
3302.738464	293482.904198	52.107252
3301.998878	293310.301205	52.112257
3301.056993	293141.728468	52.117261
3300.367984	292972.377056	52.122266
3299.879300	292812.060255	52.127271
3299.066922	292631.547892	52.132276
3298.910600	292461.322368	52.137281
3297.961437	292292.495505	52.142285
3297.183190	292112.486708	52.147290
3296.312155	291958.622175	52.152295
3295.641651	291777.628327	52.157300
3295.199501	291610.350731	52.162305
3294.011126	291460.661840	52.167309
3293.981915	291267.647353	52.172314
3293.274813	291093.076654	52.177319
3291.894524	290917.262534	52.182324
3292.156389	290757.997219	52.187329
3290.930962	290580.859533	52.192333
3290.501513	290426.440363	52.197338
3289.725592	290258.705356	52.202343
3289.174990	290107.386767	52.207348
3288.840636	289935.914367	52.212353
3288.167944	289768.366482	52.217357
3287.402701	289590.136670	52.222362
3286.735875	289416.857403	52.227367
3285.765842	289258.422795	52.232372
3284.982469	289084.423203	52.237377
3284.237195	288919.356698	52.242381
3284.131049	288752.380790	52.247386
3283.171639	288584.801193	52.252391
3282.261061	288419.327616	52.257396
3281.806187	288251.922715	52.262401
3281.009882	288099.444992	52.267405
3280.549539	287913.296402	52.272410
3279.411885	287746.712346	52.277415
3278.855531	287596.641359	52.282420
3278.818328	287418.906388	52.287425
3277.799678	287257.524202	52.292429
3277.288823	287088.828711	52.297434
3276.394681	286926.815448	52.302439
3275.704915	286751.297208	52.307444
3275.166187	286585.865797	52.312449
3274.392454	286419.376360	52.317453
3273.907357	286249.403007	52.322458
3273.086689	286088.651160	52.327463
3272.155026	285923.179744	52.332468
3271.710713	285766.876079	52.337473
3270.919037	285594.913494	52.342477
3270.271754	285431.154190	52.347482
3269.596845	285270.277087	52.352487
3268.990297	285107.682746	52.357492
3268.448015	284954.603255	52.362497
3267.689074	284783.373738	52.367501
3267.278103	284616.189482	52.372506
3266.638061	284454.695329	52.377511
3265.278860	284281.344847	52.382516
3265.159947	284120.557656	52.387521
3264.399288	283955.109379	52.392525
3263.778200	283793.841217	52.397530
3263.150228	283630.434765	52.402535
3262.268762	283476.415189	52.407540
3261.857189	283294.459017	52.412545
3260.838929	283147.795829	52.417549
3260.580316	282970.476034	52.422554
3259.614744	282820.697300	52.427559
3258.980016	282656.247423	52.432564
3258.667866	282480.209356	52.437569
3257.638726	282329.956656	52.442573
3257.162622	282147.730174	52.447578
3256.238529	281995.499719	52.452583
3255.512789	281835.699242	52.457588
3255.308477	281657.224399	52.462593
3254.280002	281524.238898	52.467597
3253.622768	281349.299308	52.472602
3253.489865	281192.766714	52.477607
3252.548976	281022.023250	52.482612
3252.112571	280857.006716	52.487617
3251.271606	280688.896074	52.492621
3250.557085	280515.289707	52.497626
3249.929281	280358.656957	52.502631
3248.855136	280186.813790	52.507636
3248.318439	280022.908094	52.512641
3247.685776	279869.255822	52.517645
3247.225562	279707.655592	52.522650
3246.433581	279535.156430	52.527655
3245.633301	279373.355260	52.532660
3245.056293	279207.061783	52.537665
3244.026500	279049.804772	52.542669
3243.507025	278889.385339	52.547674
3243.206334	278734.406973	52.552679
3242.315158	278568.927160	52.557684
3242.128300	278418.744271	52.562689
3240.912343	278258.842438	52.567693
3240.531951	278085.717660	52.572698
3239.640430	277930.221436	52.577703
3239.133039	277762.210392	52.582708
3238.294807	277602.044996	52.587713
3237.737942	277446.775942	52.592717
3236.872178	277279.942162	52.597722
3236.381931	277131.233392	52.602727
3235.481248	276967.665069	52.607732
3235.230306	276806.489852	52.612737
3234.424304	276653.475916	52.617741
3233.743621	276484.702683	52.622746
3233.381694	276319.470061	52.627751
3232.213278	276170.639324	52.632756
3232.037278	275999.010182	52.637761
3231.054896	275845.514761	52.642765
3230.592733	275673.778076	52.647770
3229.983407	275515.715730	52.652775
3228.985354	275355.193511	52.657780
3228.803112	275192.402887	52.662785
3227.694754	275036.864460	52.667789
3227.116497	274876.377711	52.672794
3226.416971	274706.053884	52.677799
3225.637986	274556.193751	52.682804
3225.244278	274388.877764	52.687809
3224.438890	274234.412044	52.692813
3223.989280	274063.182786	52.697818
3223.158682	273902.303040	52.702823
3222.322295	273749.574103	52.707828
3221.707360	273595.052824	52.712833
3221.285524	273425.754817	52.717837
3220.551888	273258.772838	52.722842
3220.261770	273107.995000	52.727847
3219.129103	272944.157856	52.732852
3218.813760	272782.585451	52.737857
3217.991591	272620.303727	52.742861
3217.370615	272451.088266	52.747866
3216.718587	272284.933944	52.752871
3215.856180	272130.222751	52.757876
3215.391546	271964.217104	52.762881
3214.702887	271806.447733	52.767885
3213.979231	271631.951220	52.772890
3213.168975	271469.896987	52.777895
3212.500674	271319.637630	52.782900
3212.161055	271149.002569	52.787905
3211.183608	270990.795119	52.792909
3210.547936	270831.336615	52.797914
3209.789241	270671.006213	52.802919
3209.103235	270517.438914	52.807924
3208.451139	270359.001832	52.812929
3207.605514	270208.490574	52.817933
3206.653635	270041.136145	52.822938
3206.357779	269889.060812	52.827943
3205.541390	269742.034181	52.832948
3205.428416	269578.061761	52.837953
3204.218981	269424.552035	52.842957
3204.059456	269256.333856	52.847962
3203.084968	269097.515105	52.852967
3202.348321	268952.870052	52.857972
3201.994981	268784.224235	52.862977
3201.228346	268631.612441	52.867981
3200.444943	268465.454240	52.872986
3199.646785	268319.774876	52.877991
3199.039591	268163.139470	52.882996
3198.472216	267997.074571	52.888001
3197.474246	267848.141547	52.893005
3196.840932	267691.510412	52.898010
3196.250385	267543.608148	52.903015
3195.573440	267399.055928	52.908020
3194.678325	267238.213168	52.913025
3194.221016	267089.525914	52.918029
3193.552898	266934.759701	52.923034
3192.674616	266793.677719	52.928039
3192.268660	266633.801966	52.933044
3192.054681	266474.609002	52.938049
3191.503560	266328.585521	52.943053
3190.691381	266163.400433	52.948058
3190.111121	266005.615402	52.953063
3189.179780	265843.174378	52.958068
3188.646663	265688.743796	52.963073
3187.605495	265533.756952	52.968077
3187.294954	265365.691323	52.973082
3186.623240	265218.948737	52.978087
3185.588378	265067.628477	52.983092
3185.024727	264904.824042	52.988097
3184.523957	264752.935511	52.993101
3183.760083	264599.458716	52.998106
3183.427484	264439.699555	53.003111
3182.306063	264297.052424	53.008116
3182.139913	264130.772725	53.013121
3181.221022	263984.120669	53.018125
3180.447859	263813.964158	53.023130
3179.762729	263661.850577	53.028135
3179.168605	263515.733098	53.033140
3178.920348	263357.005271	53.038145
3177.762967	263197.912004	53.043149
3177.450193	263038.303161	53.048154
3176.626070	262878.800771	53.053159
3175.785230	262736.466454	53.058164
3175.088566	262576.740306	53.063169
3174.464895	262432.079658	53.068173
3173.986067	262274.662241	53.073178
3173.288759	262119.698916	53.078183
3172.300832	261952.098683	53.083188
3171.943154	261798.355177	53.088193
3171.258894	261653.169666	53.093197
3170.309051	261493.229471	53.098202
3169.833218	261331.304284	53.103207
3168.871255	261179.694139	53.108212
3168.152907	261029.013304	53.113217
3167.468052	260889.787724	53.118221
3167.080321	260730.090101	53.123226
3166.381917	260587.530548	53.128231
3165.319004	260441.284997	53.133236
3165.161064	260288.376612	53.138241
3164.482054	260142.834510	53.143245
3163.978463	259988.452930	53.148250
3163.434580	259832.931775	53.153255
3162.847209	259681.110396	53.158260
3161.949323	259520.450052	53.163265
3161.178895	259370.848036	53.168269
3160.307066	259213.443614	53.173274
3159.911354	259060.853724	53.178279
3159.316459	258912.293845	53.183284
3158.603472	258754.839115	53.188289
3158.224828	258606.550817	53.193293
3157.251787	258442.974306	53.198298
3156.647117	258285.375407	53.203303
3155.848444	258134.021368	53.208308
3155.161773	257988.863756	53.213313
3153.976188	257847.095943	53.218317
3153.469944	257690.526038	53.223322
3153.117838	257536.605925	53.228327
3152.211301	257398.588876	53.233332
3151.798339	257238.260822	53.238337
3150.929391	257100.467217	53.243341
3150.210498	256950.782188	53.248346
3150.005835	256803.384351	53.253351
3149.033789	256660.386541	53.258356
3148.487087	256501.710095	53.263361
3147.385614	256367.646502	53.268365
3146.788113	256204.292343	53.273370
3146.456402	256053.426118	53.278375
3145.544586	255914.061093	53.283380
3145.301953	255757.629140	53.288385
3144.593403	255614.310210	53.293389
3143.826573	255468.224686	53.298394
3143.103197	255320.375161	53.303399
3142.649758	255159.876820	53.308404
3141.950351	255012.151065	53.313409
3141.057289	254865.780351	53.318413
3140.440878	254717.939815	53.323418
3139.967391	254573.387487	53.328423
3139.061217	254416.755977	53.333428
3138.440941	254257.201588	53.338433
3137.725059	254118.774564	53.343437
3136.905195	253977.741000	53.348442
3136.458639	253818.159490	53.353447
3135.817024	253672.743108	53.358452
3135.231528	253516.418137	53.363457
3134.443547	253374.208509	53.368461
3133.949941	253219.982999	53.373466
3133.340211	253078.407532	53.378471
3132.537902	252932.176760	53.383476
3131.870966	252776.170913	53.388481
3130.997748	252636.904031	53.393485
3130.606137	252492.085702	53.398490
3130.049141	252350.400600	53.403495
3128.995639	252201.688976	53.408500
3128.568313	252046.307992	53.413505
3127.820292	251898.261354	53.418509
3126.988168	251747.019358	53.423514
3126.449555	251587.556272	53.428519
3125.860960	251454.841148	53.433524
3125.261404	251298.545834	53.438529
3124.297028	251163.700281	53.443533
3123.697889	251006.157315	53.448538
3122.894517	250869.172803	53.453543
3122.132006	250723.039478	53.458548
3121.820136	250572.378345	53.463553
3120.961073	250436.268867	53.468557
3120.266612	250293.181130	53.473562
3119.716994	250146.046912	53.478567
3118.610975	250006.080523	53.483572
3118.315997	249862.497025	53.488577
3117.776011	249724.020225	53.493581
3117.010002	249587.005425	53.498586
3116.577707	249441.737800	53.503591
3115.705346	249295.062907	53.508596
3115.275896	249149.260314	53.513601
3114.124696	249011.874052	53.518605
3113.506720	248860.346207	53.523610
3113.102217	248710.669226	53.528615
3112.547714	248570.362194	53.533620
3111.932283	248422.526972	53.538625
3111.165970	248284.774868	53.543629
3110.642278	248144.896281	53.548634
3109.989044	247994.699122	53.553639
3109.107483	247845.709684	53.558644
3108.706261	247701.763043	53.563649
3107.647184	247561.154824	53.568653
3107.072747	247409.647032	53.573658
3106.385137	247275.143058	53.578663
3105.689614	247134.426790	53.583668
3105.310136	246988.949464	53.588673
3104.549077	246841.419010	53.593677
3104.138703	246697.551219	53.598682
3103.271310	246550.394417	53.603687
3102.395607	246402.653373	53.608692
3102.061487	246253.146042	53.613697
3101.259253	246112.778735	53.618701
3100.545372	245968.526808	53.623706
3099.942882	245817.509013	53.628711
3098.750228	245678.477216	53.633716
3098.267654	245529.758131	53.638721
3097.606185	245390.260584	53.643725
3096.954848	245247.349197	53.648730
3095.966538	245116.460072	53.653735
3095.514719	244985.206053	53.658740
3095.188798	244835.240603	53.663745
3094.453793	244697.308808	53.668749
3093.890756	244549.978678	53.673754
3093.226436	244404.167199	53.678759
3092.370733	244272.697687	53.683764
3091.920449	244129.093592	53.688769
3091.311884	243991.117067	53.693773
3090.402095	243838.647702	53.698778
3089.748275	243701.442606	53.703783
3088.976638	243561.302341	53.708788
3088.754929	243421.737293	53.713793
3087.634413	243287.840578	53.718797
3087.301141	243137.750933	53.723802
3086.943774	242997.800382	53.728807
3086.017634	242853.203500	53.733812
3085.358991	242711.416536	53.738817
3084.717812	242568.913950	53.743821
3084.026503	242412.591988	53.748826
3083.318373	242263.555857	53.753831
3082.328166	242123.782842	53.758836
3082.047074	241977.531545	53.763841
3081.467707	241844.365628	53.768845
3080.798942	241701.002616	53.773850
3079.985711	241556.796835	53.778855
3079.172443	241410.146619	53.783860
3078.660238	241262.506741	53.788865
3077.957446	241122.383828	53.793869
3077.509789	240982.424419	53.798874
3076.648375	240827.761176	53.803879
3076.051787	240695.617855	53.808884
3075.246288	240552.303337	53.813889
3074.772996	240409.140135	53.818893
3073.882793	240263.598501	53.823898
3073.390667	240125.124100	53.828903
3072.757679	239982.241346	53.833908
3072.227865	239833.078199	53.838913
3071.487110	239697.801250	53.843917
3070.700997	239545.877961	53.848922
3069.903374	239400.730203	53.853927
3069.023074	239269.117249	53.858932
3068.805361	239119.803790	53.863937
3067.883356	238978.572293	53.868941
3067.385331	238840.915252	53.873946
3066.824859	238701.205669	53.878951
3066.073204	238558.012472	53.883956
3065.578231	238411.977788	53.888961
3064.482934	238270.952872	53.893965
3064.118995	238131.034661	53.898970
3063.581066	237987.324568	53.903975
3062.872097	237847.283081	53.908980
3062.175692	237705.788345	53.913985
3061.423161	237556.434337	53.918989
3060.508365	237410.645694	53.923994
3060.048696	237263.257388	53.928999
3059.364955	237123.314710	53.934004
3058.709920	236981.941704	53.939009
3057.819286	236851.046297	53.944013
3057.552841	236714.093760	53.949018
3056.805718	236558.476238	53.954023
3055.999665	236428.128173	53.959028
3055.469244	236279.377408	53.964033
3054.614623	236138.520938	53.969037
3053.926602	235996.950777	53.974042
3053.216387	235854.493102	53.979047
3052.644905	235708.346933	53.984052
3052.503767	235565.468566	53.989057
3051.569286	235430.151265	53.994061
3050.764741	235283.762496	53.999066
3050.139177	235136.097909	54.004071
3049.324133	235002.493782	54.009076
3048.700587	234854.294561	54.014081
3048.090106	234718.315819	54.019085
3047.427516	234581.581615	54.024090
3046.729990	234443.809142	54.029095
3045.963915	234314.501452	54.034100
3045.565653	234156.387940	54.039105
3044.756077	234020.823613	54.044109
3043.952018	233878.791006	54.049114
3043.585235	233740.152354	54.054119
3042.434780	233603.293024	54.059124
3042.008658	233466.701186	54.064129
3041.207517	233337.222099	54.069133
3040.390216	233188.928743	54.074138
3040.034108	233052.962978	54.079143
3039.118848	232922.560391	54.084148
3038.967467	232775.155320	54.089153
3038.129655	232646.039449	54.094157
3037.158577	232496.676614	54.099162
3036.897243	232353.949256	54.104167
3035.982054	232218.455113	54.109172
3035.274905	232078.421377	54.114177
3034.493908	231954.262647	54.119181
3034.173615	231814.269924	54.124186
3033.601437	231678.111174	54.129191
3032.779835	231547.084571	54.134196
3032.101549	231389.707448	54.139201
3031.462048	231256.411752	54.144205
3030.779563	231112.938163	54.149210
3030.366416	230975.584016	54.154215
3029.482173	230845.994210	54.159220
3028.687674	230697.166490	54.164225
3027.935393	230557.804221	54.169229
3027.516133	230430.356610	54.174234
3026.898346	230289.929523	54.179239
3026.236372	230153.074322	54.184244
3025.973331	230007.957449	54.189249
3025.145809	229863.388473	54.194253
3024.054718	229718.428599	54.199258
3023.633780	229573.464734	54.204263
3022.502460	229429.861175	54.209268
3021.859567	229287.351778	54.214273
3021.249855	229154.818332	54.219277
3020.372047	229013.696030	54.224282
3019.838572	228883.009628	54.229287
3019.231513	228758.394917	54.234292
3018.760468	228622.861328	54.239297
3017.645807	228486.716904	54.244301
3017.161088	228352.458975	54.249306
3016.630293	228220.245460	54.254311
3015.771930	228079.834519	54.259316
3015.148556	227947.967074	54.264321
3014.303464	227826.370362	54.269325
3013.651969	227690.688574	54.274330
3013.328164	227562.389803	54.279335
3012.321709	227429.285278	54.284340
3012.060490	227300.289545	54.289345
3011.321558	227176.003543	54.294349
3010.553127	227042.454574	54.299354
3010.089281	226916.775976	54.304359
3009.574188	226777.764134	54.309364
3008.886570	226629.715745	54.314369
3008.255322	226500.423361	54.319373
3007.408822	226363.463348	54.324378
3006.687230	226224.243239	54.329383
3005.730937	226098.669289	54.334388
3005.191749	225951.018721	54.339393
3004.597797	225828.621338	54.344397
3003.662355	225687.793776	54.349402
3003.373708	225563.999048	54.354407
3002.579391	225437.751227	54.359412
3002.269443	225304.196146	54.364417
3001.469367	225179.782795	54.369421
3000.691602	225042.279444	54.374426
3000.372507	224902.514130	54.379431
2999.400275	224771.050676	54.384436
2998.973026	224633.912634	54.389441
2998.196156	224503.233424	54.394445
2997.368469	224369.876420	54.399450
2996.850096	224229.647352	54.404455
2996.104389	224100.084119	54.409460
2995.202623	223965.428325	54.414465
2994.698737	223835.890895	54.419469
2994.032133	223710.720367	54.424474
2993.604671	223570.172558	54.429479
2992.859271	223442.685344	54.434484
2992.191687	223303.958218	54.439489
2991.528468	223171.799283	54.444493
2990.587592	223038.106018	54.449498
2990.211891	222913.259885	54.454503
2989.690355	222772.855705	54.459508
2988.757516	222628.888890	54.464513
2988.132755	222501.855130	54.469517
2987.599078	222371.077335	54.474522
2987.069650	222228.218552	54.479527
2986.084169	222103.190208	54.484532
2985.696278	221966.725295	54.489537
2985.130777	221831.485334	54.494541
2984.383781	221697.712797	54.499546
2983.653991	221557.954840	54.504551
2982.753962	221429.591644	54.509556
2982.557351	221288.769602	54.514561
2981.940094	221164.219164	54.519565
2981.002152	221016.157293	54.524570
2980.487165	220882.833202	54.529575
2979.333613	220743.411167	54.534580
2979.135517	220612.379625	54.539585
2978.167110	220485.416390	54.544589
2977.463398	220351.372092	54.549594
2977.022521	220209.292356	54.554599
2976.238362	220087.366947	54.559604
2975.861979	219946.066733	54.564609
2974.850519	219812.861355	54.569613
2974.338715	219682.912205	54.574618
2973.765353	219543.986146	54.579623
2972.911191	219409.598238	54.584628
2972.001301	219271.833421	54.589633
2971.497661	219143.335078	54.594637
2970.823248	219013.260118	54.599642
2970.356790	218886.143831	54.604647
2969.313391	218750.590565	54.609652
2968.774320	218605.538157	54.614657
2968.026653	218471.058768	54.619661
2967.256231	218349.108655	54.624666
2967.118784	218206.513837	54.629671
2965.795668	218076.428715	54.634676
2965.516120	217957.825676	54.639681
2964.979315	217824.421555	54.644685
2964.328032	217694.485359	54.649690
2963.692709	217561.071874	54.654695
2962.957395	217431.760455	54.659700
2962.482773	217295.738063	54.664705
2961.787092	217170.366812	54.669709
2960.912228	217036.113957	54.674714
2960.330059	216904.360789	54.679719
2959.640288	216771.937551	54.684724
2959.234431	216631.475947	54.689729
2958.271563	216502.635059	54.694733
2957.465177	216376.939092	54.699738
2957.057644	216240.284439	54.704743
2955.890055	216121.214135	54.709748
2955.714954	215977.369690	54.714753
2954.753267	215856.816183	54.719757
2954.355571	215727.225389	54.724762
2953.834258	215597.399840	54.729767
2952.903223	215470.566972	54.734772
2952.749335	215333.479394	54.739777
2951.571834	215201.263695	54.744781
2951.056562	215066.066777	54.749786
2950.319374	214937.205850	54.754791
2949.485738	214808.347712	54.759796
2949.006107	214669.340147	54.764801
2948.284011	214554.007869	54.769805
2947.832130	214410.592427	54.774810
2947.285582	214275.771177	54.779815
2946.267786	214160.053632	54.784820
2945.756863	214020.186850	54.789825
2945.068436	213893.382204	54.794829
2944.594073	213760.217978	54.799834
2943.986890	213632.624548	54.804839
2942.922674	213498.854183	54.809844
2942.365796	213356.514088	54.814849
2941.771476	213227.010187	54.819853
2940.971207	213106.639745	54.824858
2940.552324	212982.887115	54.829863
2939.716326	212850.812965	54.834868
2938.883938	212717.669358	54.839873
2938.460920	212590.787033	54.844877
2937.540301	212457.759754	54.849882
2937.072523	212329.090383	54.854887
2936.306186	212208.779878	54.859892
2935.697629	212077.689535	54.864897
2935.042426	211948.923320	54.869901
2934.198023	211822.745617	54.874906
2933.863104	211685.948858	54.879911
2933.121101	211563.917454	54.884916
2932.359826	211439.738342	54.889921
2931.707797	211307.447324	54.894925
2931.050519	211180.604881	54.899930
2930.569391	211046.492742	54.904935
2929.386005	210918.499533	54.909940
2929.053738	210784.606208	54.914945
2928.560775	210666.559044	54.919949
2927.789017	210536.986855	54.924954
2927.273097	210406.699868	54.929959
2926.477611	210286.753998	54.934964
2925.727108	210149.453627	54.939969
2924.998275	210018.832060	54.944973
2924.372868	209895.805418	54.949978
2923.757410	209767.113734	54.954983
2922.692932	209651.564464	54.959988
2922.191661	209511.031465	54.964993
2921.633690	209389.942443	54.969997
2920.983815	209270.153672	54.975002
2920.432843	209146.620372	54.980007
2919.562853	209022.997830	54.985012
2919.176319	208891.739001	54.990017
2918.496348	208770.543245	54.995021
2917.648795	208634.890701	55.000026
2917.420495	208509.067614	55.005031
2916.491625	208385.022964	55.010036
2915.774982	208253.575961	55.015041
2915.353767	208128.484199	55.020045
2914.529451	208000.923830	55.025050
2914.000039	207874.869740	55.030055
2913.332508	207743.021535	55.035060
2912.690880	207612.060406	55.040065
2911.841230	207480.903415	55.045069
2911.202850	207351.304128	55.050074
2910.759337	207226.166868	55.055079
2909.894461	207106.187338	55.060084
2909.230532	206964.527853	55.065089
2908.792103	206849.253892	55.070093
2907.894196	206714.135461	55.075098
2907.199087	206577.101667	55.080103
2906.496712	206447.947195	55.085108
2906.089968	206319.166179	55.090113
2905.298566	206190.739063	55.095117
2904.769714	206063.899670	55.100122
2904.275921	205934.102422	55.105127
2903.272882	205809.107662	55.110132
2902.797832	205670.984832	55.115137
2902.106072	205553.373654	55.120141
2901.035669	205420.754466	55.125146
2900.430693	205290.161759	55.130151
2899.702694	205164.157625	55.135156
2899.049815	205043.461521	55.140161
2898.389790	204919.177954	55.145165
2897.548071	204801.235709	55.150170
2897.497328	204671.027522	55.155175
2896.603787	204555.753794	55.160180
2895.896441	204412.911104	55.165185
2895.277496	204298.510708	55.170189
2894.797497	204170.446008	55.175194
2894.143674	204040.563816	55.180199
2893.166195	203915.836368	55.185204
2892.691634	203782.681204	55.190209
2891.623404	203661.939245	55.195213
2891.094550	203541.468470	55.200218
2890.341639	203405.024029	55.205223
2889.934349	203289.701328	55.210228
2889.414614	203171.724203	55.215233
2888.595592	203050.205985	55.220237
2887.985936	202923.042729	55.225242
2887.495088	202792.030444	55.230247
2886.689094	202663.957146	55.235252
2885.893607	202535.017118	55.240257
2885.304742	202408.971617	55.245261
2884.592970	202292.999258	55.250266
2883.904991	202157.909236	55.255271
2883.099921	202038.503494	55.260276
2882.540152	201917.290291	55.265281
2881.790051	201796.731050	55.270285
2880.846238	201678.187952	55.275290
2880.138392	201547.531104	55.280295
2879.496450	201426.726485	55.285300
2879.353696	201311.213290	55.290305
2878.242572	201190.445306	55.295309
2877.517725	201066.765905	55.300314
2877.159120	200937.925864	55.305319
2876.388872	200827.883212	55.310324
2875.524432	200706.988160	55.315329
2874.985725	200595.916728	55.320333
2874.295191	200475.440044	55.325338
2873.747817	200359.331212	55.330343
2873.180536	200241.418781	55.335348
2872.646577	200120.663587	55.340353
2872.026020	199997.606373	55.345357
2871.204991	199866.144339	55.350362
2870.863377	199737.291736	55.355367
2870.010066	199627.175604	55.360372
2869.272532	199510.258849	55.365377
2868.710707	199384.114250	55.370381
2867.998899	199262.078458	55.375386
2867.308540	199125.100304	55.380391
2866.611132	199016.360504	55.385396
2866.264373	198885.296608	55.390401
2865.576496	198764.632470	55.395405
2864.710049	198642.508062	55.400410
2864.278080	198517.083004	55.405415
2863.473211	198402.584359	55.410420
2862.540060	198265.595973	55.415425
2862.121960	198149.255152	55.420429
2861.332122	198028.926962	55.425434
2860.741477	197905.768053	55.430439
2860.069732	197797.688388	55.435444
2859.453801	197660.829494	55.440449
2858.956207	197540.227105	55.445453
2857.893429	197412.296011	55.450458
2857.267825	197287.604410	55.455463
2856.537458	197178.122877	55.460468
2856.161002	197054.499423	55.465473
2855.462996	196927.962362	55.470477
2854.726595	196801.317169	55.475482
2854.176393	196682.112075	55.480487
2853.257575	196563.627299	55.485492
2852.611594	196425.974779	55.490497
2852.112168	196311.954066	55.495501
2851.234550	196201.887150	55.500506
2850.812966	196079.609236	55.505511
2850.002378	195948.842480	55.510516
2849.374647	195827.437617	55.515521
2848.578151	195706.670532	55.520525
2847.879801	195598.268853	55.525530
2847.555608	195465.695818	55.530535
2846.551904	195350.561032	55.535540
2845.968580	195227.076531	55.540545
2845.588349	195105.468785	55.545549
2844.340538	194989.215584	55.550554
2843.975655	194863.788768	55.555559
2843.175183	194745.340377	55.560564
2842.585351	194627.355142	55.565569
2842.173438	194509.901863	55.570573
2841.708714	194395.383722	55.575578
2840.814203	194275.933416	55.580583
2839.923769	194157.208009	55.585588
2839.575183	194031.551660	55.590593
2838.664523	193915.285729	55.595597
2838.142556	193799.162097	55.600602
2837.380917	193677.707274	55.605607
2836.742835	193557.047498	55.610612
2836.304191	193432.501161	55.615617
2835.146308	193324.889688	55.620621
2834.437875	193200.552065	55.625626
2834.312620	193081.822566	55.630631
2833.109248	192974.231785	55.635636
2832.627422	192849.337495	55.640641
2831.733088	192735.985436	55.645645
2831.429674	192621.509458	55.650650
2830.695214	192500.294973	55.655655
2829.923265	192376.987364	55.660660
2829.412463	192264.059148	55.665665
2828.631924	192144.379646	55.670669
2827.683962	192037.132177	55.675674
2827.509648	191920.690728	55.680679
2826.370063	191809.288149	55.685684
2825.752168	191693.222849	55.690689
2825.296793	191584.066228	55.695693
2824.408496	191456.008182	55.700698
2823.854714	191346.206077	55.705703
2823.391777	191235.359264	55.710708
2822.803867	191113.361642	55.715713
2822.256805	191002.159718	55.720717
2821.306624	190883.311750	55.725722
2821.123280	190761.772593	55.730727
2820.052792	190639.127389	55.735732
2819.467834	190527.092852	55.740737
2819.032645	190419.971338	55.745741
2818.008201	190302.777823	55.750746
2817.579539	190182.016913	55.755751
2816.725307	190075.738626	55.760756
2816.101603	189949.754680	55.765761
2815.357333	189826.003917	55.770765
2814.914223	189718.376325	55.775770
2814.556822	189597.427496	55.780775
2813.319987	189485.689488	55.785780
2812.921355	189362.686722	55.790785
2812.417333	189244.611878	55.795789
2811.782759	189127.613976	55.800794
2811.248770	188996.058613	55.805799
2810.250302	188879.704192	55.810804
2809.546499	188765.491654	55.815809
2809.078268	188650.224293	55.820813
2808.202894	188536.599271	55.825818
2808.002217	188403.771433	55.830823
2806.822067	188287.065590	55.835828
2806.302848	188161.985887	55.840833
2805.952524	188047.273843	55.845837
2805.036093	187927.601020	55.850842
2804.241210	187811.725910	55.855847
2803.453131	187692.440476	55.860852
2803.089566	187575.250877	55.865857
2802.503851	187460.106846	55.870861
2801.633992	187349.473544	55.875866
2801.268596	187225.669655	55.880871
2800.308687	187111.158249	55.885876
2799.707819	186985.789327	55.890881
2798.972477	186868.087918	55.895885
2798.122586	186752.923886	55.900890
2797.786050	186625.504026	55.905895
2796.917643	186515.228716	55.910900
2796.104099	186398.266044	55.915905
2795.439302	186283.341039	55.920909
2794.702260	186175.144836	55.925914
2794.243506	186053.127221	55.930919
2793.327596	185945.328823	55.935924
2792.747994	185830.391469	55.940929
2792.210004	185709.417779	55.945933
2791.622552	185602.624068	55.950938
2791.227994	185482.964031	55.955943
2789.940796	185368.954095	55.960948
2789.492046	185258.119237	55.965953
2788.967601	185143.581981	55.970957
2788.619434	185035.708556	55.975962
2787.974408	184910.937537	55.980967
2787.103965	184792.575956	55.985972
2786.359559	184667.426992	55.990977
2785.767925	184555.738727	55.995981
2784.812288	184439.948548	56.000986
2784.288936	184320.655478	56.005991
2783.613453	184222.020564	56.010996
2782.744408	184098.457641	56.016001
2782.247101	183983.562864	56.021005
2781.353223	183867.573576	56.026010
2781.101945	183746.356234	56.031015
2780.348360	183642.061396	56.036020
2779.655218	183534.513380	56.041025
2779.187498	183419.284633	56.046029
2778.377449	183291.567588	56.051034
2778.247095	183176.311484	56.056039
2777.170202	183059.551889	56.061044
2776.758160	182940.779180	56.066049
2776.298150	182821.403793	56.071053
2775.334950	182703.405944	56.076058
2774.750502	182577.156290	56.081063
2773.914365	182458.948165	56.086068
2773.287300	182339.028121	56.091073
2772.549789	182222.980242	56.096077
2771.765229	182110.578206	56.101082
2771.421989	181989.685568	56.106087
2770.470674	181888.186575	56.111092
2770.220537	181752.129736	56.116097
2769.556678	181629.113684	56.121101
2768.410168	181515.231347	56.126106
2767.985841	181384.431334	56.131111
2767.191674	181279.741509	56.136116
2766.776684	181164.866529	56.141121
2766.098668	181052.056036	56.146125
2765.051737	180925.133946	56.151130
2764.795503	180804.599725	56.156135
2763.421692	180695.093143	56.161140
2762.774244	180569.190044	56.166145
2762.473584	180463.991557	56.171149
2761.408436	180353.444794	56.176154
2761.175653	180237.474952	56.181159
2760.226165	180132.074770	56.186164
2759.775289	180016.496232	56.191169
2759.054054	179902.843378	56.196173
2758.319222	179794.141015	56.201178
2757.692923	179680.702676	56.206183
2757.101910	179578.312571	56.211188
2756.551580	179462.509616	56.216193
2755.732785	179350.781662	56.221197
2755.034495	179239.976174	56.226202
2754.822650	179122.365216	56.231207
2754.106588	179013.445652	56.236212
2753.334654	178893.367398	56.241217
2752.535173	178778.712389	56.246221
2752.252370	178659.027953	56.251226
2751.489094	178544.011704	56.256231
2750.688731	178437.600008	56.261236
2749.821622	178308.329606	56.266241
2749.280478	178195.568627	56.271245
2748.664719	178087.525938	56.276250
2747.678011	177960.386972	56.281255
2747.186606	177863.708966	56.286260
2746.815687	177741.662602	56.291265
2746.092436	177628.677618	56.296269
2745.165477	177513.741013	56.301274
2744.776386	177389.180164	56.306279
2743.727448	177271.210956	56.311284
2742.999535	177167.194948	56.316289
2742.619660	177054.983878	56.321293
2741.986163	176950.699078	56.326298
2741.157337	176848.684024	56.331303
2740.165992	176725.530627	56.336308
2739.850244	176613.857515	56.341313
2739.301720	176511.722583	56.346317
2738.537540	176398.200537	56.351322
2738.337145	176274.567078	56.356327
2737.337112	176163.359709	56.361332
2736.530735	176047.416034	56.366337
2735.959242	175932.516572	56.371341
2734.888374	175810.942922	56.376346
2734.814156	175700.276972	56.381351
2733.628052	175589.889197	56.386356
2733.477818	175476.056248	56.391361
2733.037900	175367.204293	56.396365
2732.092884	175260.365849	56.401370
2731.548302	175129.146568	56.406375
2730.708269	175033.573363	56.411380
2730.056084	174905.729515	56.416385
2729.413814	174791.671186	56.421389
2728.580929	174684.663883	56.426394
2728.347269	174553.231881	56.431399
2727.351160	174452.483004	56.436404
2726.745189	174341.052877	56.441409
2725.937026	174217.903500	56.446413
2725.005642	174108.649500	56.451418
2724.753296	173994.900491	56.456423
2724.323137	173889.472146	56.461428
2723.500746	173769.747560	56.466433
2722.767270	173653.684746	56.471437
2721.913722	173546.747344	56.476442
2721.728610	173432.569591	56.481447
2720.731485	173322.170827	56.486452
2719.996663	173205.041231	56.491457
2719.466332	173088.629939	56.496461
2718.417219	172975.633224	56.501466
2718.153250	172856.980243	56.506471
2717.392776	172752.446606	56.511476
2716.805673	172642.557080	56.516481
2716.291682	172528.332284	56.521485
2715.770188	172411.705383	56.526490
2715.237155	172288.772750	56.531495
2714.408034	172174.331831	56.536500
2713.497791	172058.848546	56.541505
2712.793720	171939.644884	56.546509
2712.094489	171840.661485	56.551514
2711.785943	171718.203772	56.556519
2710.825757	171613.310560	56.561524
2710.630370	171492.196382	56.566529
2709.529730	171372.243362	56.571533
2709.037566	171256.925125	56.576538
2708.533443	171140.947830	56.581543
2707.661184	171039.348700	56.586548
2706.930972	170918.486349	56.591553
2706.614915	170806.804074	56.596557
2705.515518	170687.526974	56.601562
2705.164966	170576.156036	56.606567
2704.041915	170461.436064	56.611572
2703.725053	170345.978308	56.616577
2703.063593	170230.537336	56.621581
2702.246498	170109.894742	56.626586
2701.763006	170005.273717	56.631591
2700.570924	169895.029964	56.636596
2700.294716	169776.210247	56.641601
2699.584157	169659.443508	56.646605
2698.884369	169555.786289	56.651610
2698.411821	169432.725941	56.656615
2697.822557	169320.620734	56.661620
2697.313939	169197.757603	56.666625
2696.423106	169094.373512	56.671629
2695.708080	168979.402582	56.676634
2695.222954	168853.510319	56.681639
2694.501867	168745.229895	56.686644
2694.079763	168625.266955	56.691649
2693.486931	168500.448379	56.696653
2692.655771	168389.948335	56.701658
2692.119401	168273.488865	56.706663
2691.649384	168153.522290	56.711668
2690.689362	168027.962319	56.716673
2690.037888	167904.388462	56.721677
2689.262036	167787.116450	56.726682
2688.967931	167658.527518	56.731687
2687.654419	167555.939398	56.736692
2686.972203	167430.769750	56.741697
2686.673177	167323.418377	56.746701
2685.676015	167202.864394	56.751706
2685.256185	167083.262034	56.756711
2684.093960	166966.829457	56.761716
2683.921698	166857.081484	56.766721
2683.194135	166744.319171	56.771725
2682.656130	166639.792357	56.776730
2682.098092	166509.914028	56.781735
2681.356771	166399.863365	56.786740
2680.866203	166279.181244	56.791745
2680.261546	166157.360477	56.796749
2679.499436	166039.392411	56.801754
2678.867241	165912.363467	56.806759
2677.903509	165805.096334	56.811764
2677.234053	165680.083122	56.816769
2676.716811	165560.412077	56.821773
2675.854298	165453.778410	56.826778
2675.390873	165323.927389	56.831783
2674.530483	165216.594733	56.836788
2674.009020	165097.078442	56.841793
2673.619025	164988.667431	56.846797
2672.707263	164870.942964	56.851802
2672.089899	164749.662885	56.856807
2671.508377	164639.172555	56.861812
2670.939624	164512.468974	56.866817
2670.294739	164390.342543	56.871821
2669.535190	164282.360900	56.876826
2668.835860	164152.614970	56.881831
2668.146760	164036.790564	56.886836
2667.362353	163923.308423	56.891841
2666.711603	163801.337470	56.896845
2666.220483	163685.342954	56.901850
2665.682814	163564.778921	56.906855
2664.700281	163443.599181	56.911860
2664.167515	163322.501165	56.916865
2663.610540	163215.558617	56.921869
2662.771237	163099.557566	56.926874
2662.197584	162972.834695	56.931879
2661.917843	162849.511297	56.936884
2660.650808	162737.012056	56.941889
2660.141114	162617.908895	56.946893
2659.477741	162499.478903	56.951898
2658.543620	162381.371908	56.956903
2657.689452	162272.928110	56.961908
2657.070427	162154.911796	56.966913
2656.723937	162038.874229	56.971917
2655.869898	161932.758118	56.976922
2655.385237	161811.428711	56.981927
2654.595840	161700.001313	56.986932
2653.889195	161582.725464	56.991937
2653.603158	161475.859596	56.996941
2652.842047	161364.772039	57.001946
2652.146463	161242.015895	57.006951
2651.416844	161133.288838	57.011956
2650.824648	161015.348325	57.016961
2650.462854	160891.866680	57.021965
2649.409810	160777.585227	57.026970
2648.972750	160656.137796	57.031975
2648.431736	160545.145071	57.036980
2647.943938	160419.231324	57.041985
2647.105373	160301.027101	57.046989
2646.491104	160189.030025	57.051994
2645.871785	160052.776991	57.056999
2644.941150	159945.191501	57.062004
2644.248407	159821.956732	57.067009
2643.760381	159698.918800	57.072013
2642.917303	159590.100055	57.077018
2642.522255	159466.984639	57.082023
2641.851133	159353.562649	57.087028
2640.679280	159234.817307	57.092033
2640.403395	159106.993155	57.097037
2639.575270	158993.698914	57.102042
2639.159826	158864.588323	57.107047
2638.335406	158755.705659	57.112052
2637.556584	158641.565702	57.117057
2637.058555	158524.966195	57.122061
2636.180247	158404.524512	57.127066
2635.956270	158277.534224	57.132071
2634.925226	158177.661294	57.137076
2634.067890	158058.628600	57.142081
2633.532005	157941.846364	57.147085
2632.838469	157816.788203	57.152090
2632.439746	157699.921490	57.157095
2631.790391	157595.527679	57.162100
2631.149306	157464.843573	57.167105
2630.708831	157352.434002	57.172109
2629.742631	157236.968149	57.177114
2629.521262	157104.172225	57.182119
2628.575977	156987.064014	57.187124
2627.846926	156862.053089	57.192129
2627.395972	156744.892807	57.197133
2626.501701	156621.841186	57.202138
2626.157201	156499.808850	57.207143
2625.354902	156381.319868	57.212148
2624.794942	156261.661535	57.217153
2624.304683	156141.509524	57.222157
2623.333189	156020.379101	57.227162
2623.174739	155887.997426	57.232167
2622.252026	155769.923721	57.237172
2621.087379	155644.922723	57.242177
2620.716525	155525.936163	57.247181
2619.729974	155405.140829	57.252186
2619.647877	155279.079839	57.257191
2618.650768	155164.909786	57.262196
2618.261545	155033.101903	57.267201
2617.467244	154915.087107	57.272205
2616.673530	154785.556080	57.277210
2616.052050	154667.209696	57.282215
2615.355985	154552.396587	57.287220
2614.448610	154432.443857	57.292225
2614.126433	154304.174657	57.297229
2613.472944	154194.936260	57.302234
2612.839291	154058.150008	57.307239
2612.137123	153939.475778	57.312244
2611.318700	153818.659510	57.317249
2610.705795	153698.624620	57.322253
2609.923704	153581.578625	57.327258
2609.418505	153453.506932	57.332263
2609.115526	153341.216015	57.337268
2608.384377	153206.431603	57.342273
2608.018073	153085.622621	57.347277
2606.871879	152967.276431	57.352282
2606.476613	152839.685404	57.357287
2605.527474	152718.054946	57.362292
2604.952198	152589.222345	57.367297
2604.503191	152466.750929	57.372301
2603.653153	152338.242477	57.377306
2602.618053	152211.772099	57.382311
2602.194811	152090.937643	57.387316
2601.759107	151975.850684	57.392321
2600.693798	151849.513590	57.397325
2600.352776	151724.841651	57.402330
2599.507659	151610.189444	57.407335
2598.963405	151418.135994	57.412340
2598.478486	151291.315071	57.417345
2598.059589	151167.674398	57.422349
2596.996151	151045.432745	57.427354
2596.953316	150911.845080	57.432359
2596.136812	150791.408192	57.437364
2595.287668	150655.381946	57.442369
2594.524320	150526.981257	57.447373
2593.775380	150399.900605	57.452378
2593.375690	150269.079299	57.457383
2592.660163	150143.926227	57.462388
2591.661607	150024.779286	57.467393
2591.354496	149884.425381	57.472397
2590.384166	149770.066402	57.477402
2589.962958	149636.213496	57.482407
2589.201880	149509.430582	57.487412
2588.567251	149383.085667	57.492417
2588.057899	149263.330227	57.497421
2586.921922	149131.664295	57.502426
2586.720376	149005.264946	57.507431
2585.831209	148878.695455	57.512436
2585.041751	148754.296628	57.517441
2584.442766	148616.510902	57.522445
2583.645908	148499.587151	57.527450
2583.149421	148360.998326	57.532455
2582.304997	148251.111064	57.537460
2581.645975	148126.757554	57.542465
2581.115109	148007.124602	57.547469
2580.238172	147880.849431	57.552474
2579.858026	147743.007381	57.557479
2579.153025	147633.303498	57.562484
2578.445662	147509.671746	57.567489
2577.843613	147376.581340	57.572493
2577.244472	147263.481489	57.577498
2576.799555	147133.734955	57.582503
2575.906579	147000.539731	57.587508
2575.428603	146878.360977	57.592513
2574.922633	146749.820278	57.597517
2574.021251	146627.506258	57.602522
2573.284177	146485.773984	57.607527
2572.445245	146370.796397	57.612532
2572.049657	146233.255664	57.617537
2571.218262	146102.494432	57.622541
2570.330293	145983.040103	57.627546
2569.613166	145865.528886	57.632551
2569.225386	145739.311851	57.637556
2568.458213	145623.842734	57.642561
2567.850161	145501.804317	57.647565
2567.083487	145369.333051	57.652570
2566.647845	145241.854838	57.657575
2566.033854	145128.205893	57.662580
2565.164415	144995.117122	57.667585
2564.780856	144876.286013	57.672589
2563.807788	144741.384867	57.677594
2563.779365	144610.400982	57.682599
2562.749875	144494.088107	57.687604
2561.995854	144365.634645	57.692609
2561.680788	144233.719313	57.697613
2560.684625	144109.460563	57.702618
2560.341755	143974.030847	57.707623
2559.703359	143846.755691	57.712628
2558.916124	143726.760376	57.717633
2558.098203	143585.104951	57.722637
2557.228086	143455.009062	57.727642
2556.807666	143330.789284	57.732647
2556.264181	143215.446181	57.737652
2555.377994	143075.951380	57.742657
2554.822365	142950.877799	57.747661
2553.898077	142827.858102	57.752666
2553.686454	142689.948147	57.757671
2553.142289	142568.152624	57.762676
2552.348001	142435.774571	57.767681
2551.973357	142304.131096	57.772685
2550.992098	142178.048082	57.777690
2550.662141	142030.604637	57.782695
2550.156294	141901.423316	57.787700
2549.179002	141773.105045	57.792705
2548.622768	141635.864373	57.797709
2547.614064	141502.634931	57.802714
2547.111809	141370.532891	57.807719
2546.251327	141243.468960	57.812724
2545.690920	141112.571630	57.817729
2545.459863	140971.623118	57.822733
2544.879783	140843.029844	57.827738
2544.214192	140694.566096	57.832743
2543.244922	140575.425226	57.837748
2542.784972	140430.525917	57.842753
2542.379035	140296.329587	57.847757
2541.714331	140159.049296	57.852762
2540.581560	140014.436503	57.857767
2540.065119	139874.491274	57.862772
2539.283877	139743.113982	57.867777
2538.766330	139612.356154	57.872781
2537.754469	139481.537480	57.877786
2537.558877	139335.026121	57.882791
2536.307413	139210.256180	57.887796
2535.593445	139090.775841	57.892801
2535.308781	138946.059228	57.897805
2534.690128	138810.340564	57.902810
2533.879626	138678.337357	57.907815
2533.144671	138548.164973	57.912820
2532.728067	138419.556221	57.917825
2532.223137	138270.354894	57.922829
2531.387158	138150.719814	57.927834
2530.653592	137997.211090	57.932839
2529.901300	137870.830421	57.937844
2529.202452	137742.256644	57.942849
2528.985366	137593.330733	57.947853
2527.764341	137466.962563	57.952858
2527.019745	137327.700732	57.957863
2526.479004	137199.663262	57.962868
2525.657533	137074.986650	57.967873
2525.108439	136938.986080	57.972877
2524.341863	136812.421667	57.977882
2524.148114	136684.420383	57.982887
2523.437806	136554.506996	57.987892
2522.321614	136425.674833	57.992897
2522.124514	136282.126194	57.997901
2521.166645	136168.489355	58.002906
2520.773476	136021.949556	58.007911
2519.950859	135886.568911	58.012916
2519.581512	135750.202395	58.017921
2518.874765	135613.686736	58.022925
2518.128395	135495.953853	58.027930
2517.453638	135344.113905	58.032935
2516.614535	135228.746953	58.037940
2516.015184	135093.944391	58.042945
2515.488174	134953.935334	58.047949
2514.733012	134828.927560	58.052954
2514.247715	134679.487402	58.057959
2513.581313	134553.780781	58.062964
2512.944970	134416.916634	58.067969
2512.501200	134272.705677	58.072973
2511.432093	134135.822539	58.077978
2510.959194	133995.123610	58.082983
2510.394657	133855.125848	58.087988
2509.400643	133726.387987	58.092993
2508.802487	133591.084171	58.097997
2508.376728	133447.738295	58.103002
2507.776750	133321.454932	58.108007
2506.949673	133184.220424	58.113012
2506.406350	133038.989855	58.118017
2506.085781	132903.175314	58.123021
2505.159295	132759.061202	58.128026
2504.360292	132613.073084	58.133031
2503.649410	132491.091653	58.138036
2502.753700	132352.881264	58.143041
2502.571468	132206.251291	58.148045
2502.023594	132076.700762	58.153050
2501.070006	131928.695643	58.158055
2500.234711	131787.734814	58.163060
2499.845741	131659.329589	58.168065
2499.404900	131516.389615	58.173069
2498.256985	131382.834699	58.178074
2497.625874	131234.426466	58.183079
2497.376748	131091.661490	58.188084
2496.314898	130960.241512	58.193089
2495.761191	130821.450961	58.198093
2495.215276	130683.358441	58.203098
2494.411722	130543.745171	58.208103
2493.672002	130404.300298	58.213108
2492.854729	130277.988781	58.218113
2492.482628	130134.066961	58.223117
2491.452229	130001.935239	58.228122
2491.144996	129861.611658	58.233127
2490.015646	129728.798359	58.238132
2489.640110	129593.846767	58.243137
2488.990823	129463.676641	58.248141
2488.266638	129313.870867	58.253146
2488.071511	129184.950945	58.258151
2487.209671	129058.728235	58.263156
2486.180378	128909.366729	58.268161
2486.046799	128775.320614	58.273165
2484.989296	128635.592073	58.278170
2484.524063	128497.205510	58.283175
2483.955738	128363.154102	58.288180
2483.220432	128218.372667	58.293185
2482.499151	128080.473291	58.298189
2482.004375	127947.491768	58.303194
2481.525503	127802.290872	58.308199
2480.641648	127663.250951	58.313204
2479.747493	127523.578370	58.318209
2479.419077	127387.283901	58.323213
2478.674170	127249.595645	58.328218
2478.173713	127105.875042	58.333223
2477.166042	126958.870170	58.338228
2476.722643	126830.572118	58.343233
2476.488869	126677.756652	58.348237
2475.294226	126537.222376	58.353242
2475.110489	126389.213711	58.358247
2473.723660	126256.178623	58.363252
2473.271610	126115.389128	58.368257
2472.791816	125962.896059	58.373261
2471.976493	125844.478127	58.378266
2471.341728	125688.709377	58.383271
2470.571569	125564.989980	58.388276
2470.189579	125422.427813	58.393281
2469.758680	125270.235671	58.398285
2469.230514	125132.942855	58.403290
2468.821930	124964.443581	58.408295
2467.676636	124838.615489	58.413300
2467.005415	124684.382161	58.418305
2466.812716	124539.356520	58.423309
2465.792012	124398.501035	58.428314
2465.254280	124245.112568	58.433319
2464.363790	124098.193568	58.438324
2463.636884	123957.750971	58.443329
2462.925827	123803.300457	58.448333
2462.208877	123662.159433	58.453338
2461.624858	123518.318787	58.458343
2460.902337	123381.256218	58.463348
2460.238330	123241.772468	58.468353
2459.807974	123085.072174	58.473357
2459.076782	122946.794221	58.478362
2458.316029	122797.703194	58.483367
2457.770604	122660.400407	58.488372
2457.190975	122504.946175	58.493377
2456.637486	122365.500299	58.498381
2455.910903	122228.393535	58.503386
2455.451296	122062.929965	58.508391
2454.531817	121911.939084	58.513396
2453.879150	121776.575179	58.518401
2453.522919	121615.072271	58.523405
2452.405129	121490.284134	58.528410
2451.948918	121327.821157	58.533415
2451.146304	121185.995874	58.538420
2450.531798	121029.705167	58.543425
2449.849111	120887.380005	58.548429
2448.896146	120753.452927	58.553434
2448.647230	120588.701643	58.558439
2448.000933	120463.107247	58.563444
2447.032569	120305.677125	58.568449
2446.527018	120160.528251	58.573453
2445.879848	120012.533247	58.578458
2445.199607	119859.046818	58.583463
2444.633464	119718.874272	58.588468
2443.931018	119566.554794	58.593473
2443.194260	119415.625525	58.598477
2442.366519	119276.353823	58.603482
2441.966916	119120.027794	58.608487
2440.783754	118995.115953	58.613492
2440.112711	118845.233348	58.618497
2439.364746	118706.948686	58.623501
2438.514386	118560.130447	58.628506
2438.181295	118425.501361	58.633511
2437.491487	118280.335086	58.638516
2437.218099	118148.338658	58.643521
2436.310773	118006.642536	58.648525
2435.914766	117862.396894	58.653530
2435.561452	117710.318658	58.658535
2434.457251	117565.196720	58.663540
2433.836411	117415.523947	58.668545
2433.074225	117269.486197	58.673549
2432.272453	117136.582169	58.678554
2431.564354	116986.075176	58.683559
2430.962828	116855.889312	58.688564
2430.393171	116711.157190	58.693569
2429.754186	116564.646926	58.698573
2428.857222	116434.827414	58.703578
2428.467807	116288.133188	58.708583
2427.798283	116149.805454	58.713588
2427.117070	116001.083592	58.718593
2426.327720	115856.917973	58.723597
2425.608584	115705.074701	58.728602
2425.432606	115577.335036	58.733607
2424.913658	115433.274944	58.738612
2424.195034	115281.294495	58.743617
2423.582709	115131.925763	58.748621
2422.686558	114994.700210	58.753626
2422.225296	114834.468688	58.758631
2421.632093	114687.378100	58.763636
2420.938640	114537.270473	58.768641
2420.376553	114392.391724	58.773645
2419.656391	114249.658691	58.778650
2418.798760	114094.718108	58.783655
2417.845977	113947.784054	58.788660
2417.382477	113800.970041	58.793665
2417.116006	113636.716878	58.798669
2416.262527	113503.624354	58.803674
2415.674068	113343.771570	58.808679
2414.952302	113201.641340	58.813684
2414.179944	113051.847060	58.818689
2413.784593	112898.617612	58.823693
2412.991710	112743.706872	58.828698
2412.489479	112587.526172	58.833703
2411.465565	112452.257754	58.838708
2410.921342	112294.752826	58.843713
2410.733643	112145.467866	58.848717
2409.425872	111996.843687	58.853722
2409.155134	111845.961761	58.858727
2408.096150	111696.417829	58.863732
2407.445215	111555.720014	58.868737
2406.938994	111398.754178	58.873741
2406.566351	111251.134867	58.878746
2405.495739	111101.133129	58.883751
2404.674187	110956.645509	58.888756
2403.854502	110809.962762	58.893761
2403.751847	110643.647371	58.898765
2402.669290	110513.031349	58.903770
2401.890471	110368.781553	58.908775
2401.773150	110220.943920	58.913780
2400.941927	110068.042267	58.918785
2400.354579	109919.126055	58.923789
2399.352500	109780.289899	58.928794
2399.002898	109632.778197	58.933799
2398.238933	109486.671991	58.938804
2397.678695	109337.298150	58.943809
2396.949630	109189.538359	58.948813
2396.073759	109035.641323	58.953818
2395.914288	108891.727205	58.958823
2394.978554	108757.347176	58.963828
2394.371133	108600.796046	58.968833
2393.963375	108452.120490	58.973837
2393.127404	108292.136720	58.978842
2392.929048	108133.455206	58.983847
2391.822735	107985.902150	58.988852
2391.166113	107848.970229	58.993857
2390.884170	107691.415265	58.998861
2389.676002	107542.091759	59.003866
2389.275820	107390.084042	59.008871
2388.404632	107226.058465	59.013876
2387.792371	107086.890416	59.018881
2387.490159	106923.842639	59.023885
2386.335136	106789.597164	59.028890
2385.869244	106620.391177	59.033895
2385.229679	106480.774147	59.038900
2384.627594	106323.716690	59.043905
2384.033190	106171.887063	59.048909
2383.278455	106023.192693	59.053914
2382.584768	105873.804354	59.058919
2382.250748	105727.754267	59.063924
2381.412263	105562.345443	59.068929
2380.753095	105415.625545	59.073933
2379.876075	105264.284273	59.078938
2379.410606	105102.600791	59.083943
2378.840954	104952.652949	59.088948
2377.729634	104797.278726	59.093953
2377.667270	104641.168226	59.098957
2376.634522	104491.652003	59.103962
2376.189809	104323.518459	59.108967
2375.307323	104183.636215	59.113972
2374.753436	104026.694142	59.118977
2374.126543	103871.096941	59.123981
2373.265946	103731.791216	59.128986
2372.835393	103570.950076	59.133991
2372.091546	103421.483647	59.138996
2371.125471	103262.810336	59.144001
2370.748834	103106.461651	59.149005
2370.403221	102954.308695	59.154010
2369.824643	102800.474500	59.159015
2369.006687	102648.436483	59.164020
2368.457203	102499.858607	59.169025
2367.893331	102323.758851	59.174029
2366.909417	102174.687338	59.179034
2366.206821	102008.983751	59.184039
2365.605011	101864.160918	59.189044
2364.605971	101706.816499	59.194049
2364.370748	101546.656077	59.199053
2363.476062	101397.924277	59.204058
2363.063447	101253.049876	59.209063
2362.421242	101082.046613	59.214068
2361.565689	100929.613460	59.219073
2361.120358	100764.391759	59.224077
2360.029828	100612.118475	59.229082
2359.709406	100462.438953	59.234087
2359.277076	100301.880701	59.239092
2358.309832	100143.273237	59.244097
2357.856279	99989.907200	59.249101
2356.921685	99835.540151	59.254106
2356.494401	99671.725200	59.259111
2355.404096	99519.801613	59.264116
2354.768834	99370.813386	59.269121
2354.285665	99209.274986	59.274125
2353.496481	99055.644914	59.279130
2352.952380	98896.534966	59.284135
2352.166890	98739.195946	59.289140
2351.482270	98603.838236	59.294145
2351.213018	98437.228972	59.299149
2350.296807	98293.176091	59.304154
2349.826625	98122.605180	59.309159
2349.106690	97972.104602	59.314164
2348.295480	97817.566692	59.319169
2347.867264	97657.717623	59.324173
2347.062186	97498.271920	59.329178
2346.536722	97344.687659	59.334183
2345.694284	97198.162867	59.339188
2345.008299	97039.963605	59.344193
2344.712395	96875.684896	59.349197
2343.512420	96729.035909	59.354202
2342.902088	96560.484031	59.359207
2342.253778	96410.775210	59.364212
2341.602102	96256.184597	59.369217
2340.901847	96095.298869	59.374221
2340.114118	95945.849893	59.379226
2339.725387	95799.890074	59.384231
2339.071883	95643.096995	59.389236
2338.372126	95489.597375	59.394241
2338.021260	95331.845266	59.399245
2337.120086	95173.908835	59.404250
2336.642619	95006.355848	59.409255
2335.535158	94866.978172	59.414260
2335.090456	94714.711729	59.419265
2334.915914	94555.117107	59.424269
2333.699405	94396.221529	59.429274
2333.003783	94228.391890	59.434279
2332.388886	94082.453755	59.439284
2331.640337	93932.409572	59.444289
2330.913884	93774.487037	59.449293
2330.404514	93623.481185	59.454298
2329.876087	93463.899760	59.459303
2329.145518	93322.842296	59.464308
2328.444505	93143.252543	59.469313
2327.808484	92995.029423	59.474317
2327.217569	92842.760923	59.479322
2326.606219	92692.747751	59.484327
2325.939966	92526.055012	59.489332
2324.950015	92381.062587	59.494337
2324.568222	92218.435948	59.499341
2323.814853	92065.165013	59.504346
2323.253068	91915.605800	59.509351
2322.359328	91760.317528	59.514356
2321.566485	91607.582317	59.519361
2321.444968	91446.961791	59.524365
2320.096890	91307.245208	59.529370
2319.600202	91144.594000	59.534375
2319.280592	90990.767215	59.539380
2318.691850	90846.513851	59.544385
2318.056080	90679.272320	59.549389
2317.659763	90528.707220	59.554394
2316.947187	90354.892740	59.559399
2315.885423	90205.234271	59.564404
2315.438523	90045.816863	59.569409
2315.010262	89874.389422	59.574413
2314.005248	89736.137446	59.579418
2313.507430	89565.256039	59.584423
2312.377252	89420.692202	59.589428
2311.963422	89268.610644	59.594433
2311.406534	89099.244844	59.599437
2310.426472	88954.438413	59.604442
2310.050014	88800.667802	59.609447
2309.264040	88640.154291	59.614452
2308.361563	88485.790977	59.619457
2308.164851	88328.673193	59.624461
2307.258182	88165.697186	59.629466
2306.672898	88014.431409	59.634471
2306.247679	87860.294847	59.639476
2305.802646	87704.355770	59.644481
2305.131117	87537.740044	59.649485
2304.234689	87379.256709	59.654490
2303.859117	87222.929743	59.659495
2303.255258	87055.527284	59.664500
2302.281912	86903.773001	59.669505
2301.727541	86725.056010	59.674509
2300.799479	86568.986248	59.679514
2300.208505	86417.035319	59.684519
2299.407880	86251.369242	59.689524
2298.719065	86099.772057	59.694529
2298.255609	85931.234125	59.699533
2297.475323	85784.071966	59.704538
2297.040128	85619.525553	59.709543
2296.461944	85456.961790	59.714548
2295.638333	85307.445411	59.719553
2295.247451	85130.059687	59.724557
2294.006052	84978.310915	59.729562
2293.563938	84815.533987	59.734567
2292.983949	84662.598677	59.739572
2292.558076	84486.453578	59.744577
2291.604099	84336.692166	59.749581
2291.056483	84189.637283	59.754586
2290.397086	84017.260148	59.759591
2289.686234	83857.955955	59.764596
2288.982425	83691.109249	59.769601
2288.343807	83541.557006	59.774605
2287.833584	83375.309592	59.779610
2286.960566	83225.245346	59.784615
2286.269431	83057.317831	59.789620
2285.768841	82903.945361	59.794625
2285.181612	82735.839151	59.799629
2284.381347	82586.642585	59.804634
2283.722270	82414.468687	59.809639
2283.044335	82257.769970	59.814644
2282.186952	82104.662751	59.819649
2281.730453	81935.059191	59.824653
2280.864084	81779.984728	59.829658
2280.365578	81626.614959	59.834663
2279.593067	81461.001080	59.839668
2279.136035	81308.444633	59.844673
2278.411713	81148.447050	59.849677
2277.696849	80983.486937	59.854682
2277.218122	80827.001880	59.859687
2276.738888	80666.297374	59.864692
2276.025663	80520.707789	59.869697
2275.597165	80343.660040	59.874701
2274.811420	80178.185246	59.879706
2274.346764	80001.025756	59.884711
2273.533513	79846.667090	59.889716
2272.789300	79683.173204	59.894721
2272.408784	79508.317641	59.899725
2271.280879	79344.703518	59.904730
2270.700604	79171.175246	59.909735
2269.916167	79010.633422	59.914740
2269.274792	78851.705070	59.919745
2268.347292	78685.833843	59.924750
2267.736852	78534.950767	59.929754
2267.112189	78361.949652	59.934759
2266.188938	78210.256789	59.939764
2265.382269	78051.006010	59.944769
2265.584775	77895.582108	59.949774
2264.404507	77739.662668	59.954778
2263.583158	77580.215121	59.959783
2262.794593	77413.527453	59.964788
2262.258185	77267.185196	59.969793
2261.761643	77105.985367	59.974798
2261.098776	76948.500895	59.979802
2260.421544	76790.329274	59.984807
2259.793693	76642.187526	59.989812
2259.280772	76482.116744	59.994817
2258.639086	76308.160004	59.999822
2257.654000	76165.419692	60.004826
2257.204177	75994.603221	60.009831
2256.763878	75844.296008	60.014836
2256.050275	75684.504125	60.019841
2255.705738	75518.243135	60.024846
2254.914815	75353.967709	60.029850
2254.226779	75186.648838	60.034855
2253.526702	75028.222185	60.039860
2252.662901	74868.967441	60.044865
2252.225710	74700.257010	60.049870
2251.544583	74530.604681	60.054874
2250.955463	74378.754467	60.059879
2250.271690	74204.391743	60.064884
2249.394809	74046.279636	60.069889
2249.046539	73880.096134	60.074894
2247.962095	73725.839660	60.079898
2247.276880	73553.066649	60.084903
2246.507985	73394.182349	60.089908
2245.933623	73226.874473	60.094913
2245.527326	73069.411323	60.099918
2244.591083	72919.584772	60.104922
2243.974549	72756.931075	60.109927
2243.631403	72581.768301	60.114932
2242.609086	72432.636902	60.119937
2242.328187	72256.732279	60.124942
2241.398004	72113.980451	60.129946
2240.765210	71939.192355	60.134951
2240.271751	71782.836452	60.139956
2239.763401	71622.848100	60.144961
2239.418932	71451.584941	60.149966
2238.355491	71285.606224	60.154970
2237.778096	71123.586831	60.159975
2237.215446	70949.835197	60.164980
2236.252402	70793.941660	60.169985
2235.733784	70627.711040	60.174990
2235.116925	70463.758715	60.179994
2234.418085	70284.935517	60.184999
2233.606515	70124.735045	60.190004
2232.628085	69965.379438	60.195009
2232.486830	69801.230524	60.200014
2231.823309	69645.013567	60.205018
2231.343658	69470.919809	60.210023
2230.678882	69294.785802	60.215028
2229.658391	69133.087457	60.220033
2229.112536	68966.387535	60.225038
2228.373679	68809.587499	60.230042
2227.830290	68627.936296	60.235047
2227.198247	68462.736413	60.240052
2226.527441	68300.767831	60.245057
2225.899073	68141.238576	60.250062
2224.853972	67971.364629	60.255066
2223.983638	67809.875123	60.260071
2223.736717	67641.828125	60.265076
2222.907325	67486.921432	60.270081
2222.335564	67325.850924	60.275086
2221.308855	67159.967909	60.280090
2220.926067	66987.619441	60.285095
2220.158914	66840.098750	60.290100
2219.344825	66677.013850	60.295105
2219.001651	66512.009588	60.300110
2218.399496	66355.863161	60.305114
2217.769169	66188.149254	60.310119
2217.342899	66031.189126	60.315124
2216.173902	65867.059143	60.320129
2215.815957	65695.142575	60.325134
2214.920077	65548.146145	60.330138
2214.778260	65373.054041	60.335143
2213.749529	65204.104246	60.340148
2212.971296	65048.502969	60.345153
2212.477295	64880.699701	60.350158
2211.488507	64714.869752	60.355162
2211.120113	64546.340271	60.360167
2210.726635	64394.615623	60.365172
2209.954030	64224.285096	60.370177
2209.578632	64068.247973	60.375182
2208.737170	63899.365494	60.380186
2208.220053	63729.201491	60.385191
2207.897149	63554.126277	60.390196
2207.018737	63376.395921	60.395201
2206.248231	63214.150414	60.400206
2205.491949	63036.596987	60.405210
2204.784085	62858.648142	60.410215
2204.050428	62702.951317	60.415220
2203.479610	62534.373626	60.420225
2202.622591	62368.555902	60.425230
2201.809730	62191.962771	60.430234
2201.326515	62017.876896	60.435239
2200.773119	61868.445459	60.440244
2199.924694	61701.486252	60.445249
2199.591269	61524.313648	60.450254
2198.745930	61360.798012	60.455258
2198.244395	61187.681890	60.460263
2197.471450	61026.731288	60.465268
2196.704286	60848.301158	60.470273
2196.173575	60680.746652	60.475278
2195.269619	60532.508352	60.480282
2194.543082	60367.368139	60.485287
2193.980188	60188.734621	60.490292
2193.220392	60027.860150	60.495297
2192.119518	59856.288476	60.500302
2191.524484	59706.418715	60.505306
2191.252213	59533.278347	60.510311
2190.777268	59376.669102	60.515316
2190.075790	59217.251556	60.520321
2189.934833	59039.065379	60.525326
2188.860398	58886.094062	60.530330
2188.356358	58700.634992	60.535335
2187.710790	58530.725148	60.540340
2186.986073	58368.517433	60.545345
2186.403116	58197.277701	60.550350
2185.466326	58028.456798	60.555354
2184.952451	57857.927708	60.560359
2184.135824	57693.477502	60.565364
2183.481314	57528.427022	60.570369
2182.947036	57345.182792	60.575374
2182.016771	57183.353556	60.580378
2181.594895	57024.334616	60.585383
2181.127784	56844.702145	60.590388
2180.451642	56688.141210	60.595393
2179.387631	56516.395227	60.600398
2178.600650	56343.249225	60.605402
2178.643767	56177.346970	60.610407
2177.700529	56005.928391	60.615412
2176.973086	55834.236668	60.620417
2176.609744	55657.634250	60.625422
2175.597571	55496.551236	60.630426
2174.856763	55328.923393	60.635431
2174.189588	55156.342387	60.640436
2173.181083	54993.475259	60.645441
2172.769877	54833.309074	60.650446
2172.284448	54669.026449	60.655450
2171.802122	54488.201173	60.660455
2170.962270	54336.024757	60.665460
2170.358752	54162.411465	60.670465
2169.943241	53983.226078	60.675470
2168.920327	53826.665549	60.680474
2168.368334	53643.575087	60.685479
2167.703106	53489.302294	60.690484
2167.100258	53309.093256	60.695489
2166.878585	53141.067801	60.700494
2165.907536	52971.422497	60.705498
2165.524363	52802.489213	60.710503
2164.860220	52636.003637	60.715508
2163.888069	52458.703025	60.720513
2163.259149	52280.004986	60.725518
2162.453708	52106.959172	60.730522
2161.463325	51934.874572	60.735527
2161.150381	51768.024898	60.740532
2160.411839	51600.231834	60.745537
2159.522853	51435.365496	60.750542
2158.888732	51265.834668	60.755546
2158.608599	51081.698812	60.760551
2157.937108	50927.034477	60.765556
2156.944622	50761.314381	60.770561
2156.833223	50581.459631	60.775566
2155.972385	50423.232511	60.780570
2155.110928	50246.629036	60.785575
2154.578865	50082.076030	60.790580
2153.858764	49907.604770	60.795585
2153.248802	49727.701672	60.800590
2152.396349	49566.785437	60.805594
2151.575784	49392.468029	60.810599
2151.177632	49224.504062	60.815604
2150.251831	49061.927374	60.820609
2149.957740	48897.736665	60.825614
2149.228395	48731.708986	60.830618
2148.690944	48563.523460	60.835623
2147.826623	48391.971798	60.840628
2147.084784	48215.603606	60.845633
2146.703390	48040.350404	60.850638
2145.741429	47884.629295	60.855642
2145.320637	47703.634868	60.860647
2144.756589	47537.759818	60.865652
2143.722564	47369.715037	60.870657
2143.833481	47182.138121	60.875662
2142.747287	47034.564006	60.880666
2142.078495	46855.395300	60.885671
2141.270153	46686.985945	60.890676
2140.628757	46507.455851	60.895681
2140.499292	46340.061825	60.900686
2139.407679	46169.586336	60.905690
2138.681821	45990.906784	60.910695
2137.899846	45828.080890	60.915700
2137.237255	45658.260291	60.920705
2136.917623	45487.336868	60.925710
2135.711069	45315.942245	60.930714
2135.085346	45145.747565	60.935719
2134.763009	44978.311763	60.940724
2133.891136	44811.515064	60.945729
2133.237982	44633.043439	60.950734
2132.284615	44473.824871	60.955738
2131.910103	44303.193743	60.960743
2131.084060	44139.283688	60.965748
2130.263603	43973.151015	60.970753
2129.845218	43804.818271	60.975758
2129.173179	43646.274223	60.980762
2128.383308	43476.197820	60.985767
2128.100574	43304.878850	60.990772
2127.226567	43150.122037	60.995777
2126.906971	42984.804847	61.000782
2125.889523	42815.577451	61.005786
2125.442235	42632.486209	61.010791
2125.135403	42468.405237	61.015796
2123.859923	42297.566825	61.020801
2123.591803	42122.200092	61.025806
2122.820999	41949.469947	61.030810
2122.018109	41780.496945	61.035815
2121.530406	41621.278192	61.040820
2120.820198	41435.275314	61.045825
2120.457349	41266.983800	61.050830
2119.268705	41109.847804	61.055834
2119.018268	40932.634287	61.060839
2118.197936	40759.598286	61.065844
2117.369699	40600.417743	61.070849
2116.967476	40415.780965	61.075854
2116.185173	40259.924211	61.080858
2115.418457	40081.704249	61.085863
2114.884987	39917.727886	61.090868
2114.328977	39740.551492	61.095873
2113.829741	39568.956322	61.100878
2112.821605	39392.656786	61.105882
2112.060983	39233.903518	61.110887
2111.683921	39057.910438	61.115892
2110.810165	38884.279098	61.120897
2110.146578	38718.720925	61.125902
2109.595824	38546.704787	61.130906
2109.079928	38372.348495	61.135911
2108.268997	38204.498161	61.140916
2107.117355	38051.309522	61.145921
2107.080248	37867.447067	61.150926
2106.014178	37707.989909	61.155930
2105.440310	37531.152396	61.160935
2104.787037	37354.379916	61.165940
2104.071740	37201.806278	61.170945
2103.749607	37021.764952	61.175950
2102.933714	36860.248160	61.180954
2102.161888	36685.554736	61.185959
2101.919234	36513.450360	61.190964
2100.874077	36349.796797	61.195969
2100.731558	36162.424434	61.200974
2099.742955	36010.918104	61.205978
2099.027489	35828.745529	61.210983
2098.758296	35653.875614	61.215988
2097.547469	35486.463548	61.220993
2097.040598	35306.003686	61.225998
2096.196463	35148.727729	61.231002
2095.882624	34979.838183	61.236007
2094.810703	34808.227439	61.241012
2094.186105	34642.309669	61.246017
2093.911067	34457.006680	61.251022
2093.230629	34290.976416	61.256026
2092.272768	34113.550000	61.261031
2091.488181	33962.047279	61.266036
2090.967973	33785.021129	61.271041
2090.309428	33608.274826	61.276046
2089.537078	33456.942286	61.281050
2089.046059	33286.166912	61.286055
2088.492776	33117.533377	61.291060
2087.388794	32947.261727	61.296065
2087.047855	32778.986689	61.301070
2086.061954	32614.224235	61.306074
2085.460319	32439.760050	61.311079
2084.808861	32270.393815	61.316084
2083.656414	32115.050664	61.321089
2083.680287	31948.481771	61.326094
2082.733188	31785.401145	61.331098
2082.345061	31612.025836	61.336103
2081.703766	31453.455473	61.341108
2080.561992	31292.578533	61.346113
2080.372700	31118.832412	61.351118
2079.738484	30957.029720	61.356122
2079.101681	30791.677093	61.361127
2078.643677	30626.398883	61.366132
2077.646448	30452.129151	61.371137
2077.008921	30290.384125	61.376142
2076.016038	30130.108009	61.381146
2075.363472	29950.676111	61.386151
2075.169136	29790.818536	61.391156
2074.166823	29631.774846	61.396161
2073.666199	29460.094340	61.401166
2073.318187	29300.744664	61.406170
2072.382406	29143.074438	61.411175
2071.589481	28971.409125	61.416180
2070.782660	28800.251802	61.421185
2070.578362	28624.984728	61.426190
2069.719569	28469.673829	61.431194
2068.747645	28297.672779	61.436199
2068.078824	28136.086807	61.441204
2067.457625	27975.851912	61.446209
2067.018873	27816.365311	61.451214
2066.171270	27644.141361	61.456218
2065.457335	27503.596787	61.461223
2064.604773	27326.447474	61.466228
2064.037707	27173.915382	61.471233
2063.391113	26998.004690	61.476238
2062.566717	26849.832172	61.481242
2062.112996	26686.277250	61.486247
2061.562148	26530.991389	61.491252
2060.467027	26373.235207	61.496257
2060.256673	26220.264575	61.501262
2059.652922	26053.594112	61.506266
2058.991333	25896.708923	61.511271
2058.419469	25730.938679	61.516276
2057.876483	25572.492244	61.521281
2057.310174	25393.955628	61.526286
2056.230784	25242.945496	61.531290
2055.672443	25076.640468	61.536295
2055.307181	24907.402669	61.541300
2054.287737	24758.393526	61.546305
2053.680977	24582.010177	61.551310
2053.275516	24425.736841	61.556314
2052.199470	24272.211430	61.561319
2051.272255	24103.079223	61.566324
2050.767344	23946.163020	61.571329
2050.313324	23783.765433	61.576334
2049.474347	23632.300431	61.581338
2048.555048	23476.743359	61.586343
2048.182766	23308.219330	61.591348
2047.197898	23162.968122	61.596353
2046.768945	23002.472850	61.601358
2045.916807	22855.418804	61.606362
2045.424406	22703.876859	61.611367
2044.607834	22537.203442	61.616372
2043.838945	22389.215078	61.621377
2043.263850	22229.089569	61.626382
2042.400754	22091.830692	61.631386
2041.707899	21942.000215	61.636391
2041.238809	21783.192855	61.641396
2040.244510	21649.210139	61.646401
2039.516836	21487.392720	61.651406
2038.801995	21347.861784	61.656410
2038.459834	21197.276857	61.661415
2037.586508	21055.022870	61.666420
2036.749047	20917.595654	61.671425
2036.105728	20761.265512	61.676430
2035.248473	20632.673238	61.681434
2034.514291	20494.466705	61.686439
2033.991468	20343.643471	61.691444
2033.005510	20216.421143	61.696449
2032.185141	20078.678412	61.701454
2031.491778	19949.642557	61.706458
2030.387625	19823.445223	61.711463
2029.715883	19691.554480	61.716468
2028.840763	19578.895048	61.721473
2028.294590	19457.887351	61.726478
2027.507206	19349.921245	61.731482
2026.429835	19246.712573	61.736487
2025.770722	19122.497323	61.741492
2024.527591	19028.248998	61.746497
2023.503875	18942.163153	61.751502
2022.571061	18844.136207	61.756506
2021.951509	18757.768171	61.761511
2020.679048	18667.543298	61.766516
2019.370668	18599.382621	61.771521
2018.318750	18523.713264	61.776526
2017.684624	18465.063635	61.781530
2016.991499	18408.642230	61.786535
2016.479698	18346.467467	61.791540
2015.345115	18297.088579	61.796545
2014.973487	18234.230104	61.801550
2014.464364	18188.556425	61.806554
2013.647413	18124.277500	61.811559
2013.353771	18072.768691	61.816564
2012.348218	18018.448345	61.821569
2012.205381	17955.740981	61.826574
2011.429760	17909.800190	61.831578
2010.850567	17838.947813	61.836583
2010.158096	17784.705294	61.841588
2009.825301	17721.557369	61.846593
2009.334946	17650.591502	61.851598
2008.416910	17603.797623	61.856602
2007.817202	17530.430047	61.861607
2007.645427	17477.959000	61.866612
2006.488542	17419.529299	61.871617
2006.283339	17347.979639	61.876622
2005.361158	17297.538938	61.881626
2004.671635	17230.159097	61.886631
2004.186777	17165.216146	61.891636
2003.417745	17101.273084	61.896641
2002.755362	17036.989730	61.901646
2001.985550	16987.316386	61.906650
2001.397006	16908.285891	61.911655
2000.849649	16853.390364	61.916660
1999.979050	16796.445140	61.921665
1999.967841	16727.316649	61.926670
1998.942324	16674.766760	61.931674
1998.235503	16618.708656	61.936679
1997.801328	16551.714519	61.941684
1997.056883	16493.532083	61.946689
1996.340759	16422.950441	61.951694
1995.565678	16362.018277	61.956698
1994.978167	16300.767898	61.961703
1994.183886	16232.212258	61.966708
1993.672822	16188.983731	61.971713
1993.076335	16110.221420	61.976718
1992.500723	16048.390222	61.981722
1991.569342	15997.720424	61.986727
1991.289296	15933.787074	61.991732
1990.551916	15878.652677	61.996737
1990.104125	15804.317908	62.001742
1988.969195	15736.515969	62.006746
1988.683990	15687.256590	62.011751
1988.116358	15618.344901	62.016756
1987.458961	15568.418060	62.021761
1986.863554	15481.216514	62.026766
1986.144078	15429.495528	62.031770
1985.285549	15361.884996	62.036775
1984.773194	15305.728891	62.041780
1983.880603	15245.545325	62.046785
1983.463155	15167.602836	62.051790
1982.940490	15118.986050	62.056794
1981.888041	15043.954682	62.061799
1981.547376	14982.269245	62.066804
1980.810098	14920.218355	62.071809
1980.299711	14846.791269	62.076814
1979.504555	14787.792875	62.081818
1979.171727	14719.845236	62.086823
1978.456965	14666.650356	62.091828
1977.268925	14593.577587	62.096833
1977.009358	14524.187649	62.101838
1976.246629	14472.107114	62.106842
1975.143061	14410.501366	62.111847
1974.713765	14335.618823	62.116852
1973.798967	14275.578141	62.121857
1973.480151	14223.769719	62.126862
1972.729239	14161.286363	62.131866
1971.962627	14099.568310	62.136871
1971.474251	14032.058398	62.141876
1970.805959	13980.720099	62.146881
1970.560878	13906.207773	62.151886
1969.481065	13844.784591	62.156890
1968.748940	13788.103195	62.161895
1968.491756	13718.866672	62.166900
1967.717109	13675.584482	62.171905
1967.026288	13601.150214	62.176910
1966.371011	13552.532134	62.181914
1965.880323	13469.266107	62.186919
1965.349708	13417.246045	62.191924
1964.392646	13352.881667	62.196929
1963.935010	13280.542466	62.201934
1963.024312	13215.029810	62.206938
1962.364606	13161.328335	62.211943
1961.949332	13078.962450	62.216948
1961.129551	13029.441068	62.221953
1960.608703	12955.807621	62.226958
1959.622304	12906.073785	62.231962
1959.057474	12833.741687	62.236967
1958.547838	12787.320279	62.241972
1957.743029	12721.371947	62.246977
1957.326397	12652.288877	62.251982
1956.547844	12597.602729	62.256986
1955.746675	12529.268969	62.261991
1955.121207	12459.844898	62.266996
1954.321905	12414.212172	62.272001
1953.800994	12343.207445	62.277006
1953.215923	12289.138168	62.282010
1952.815507	12222.892464	62.287015
1952.017330	12145.705542	62.292020
1951.191799	12097.525033	62.297025
1950.630858	12014.380605	62.302030
1949.666588	11967.327051	62.307034
1949.061717	11905.948894	62.312039
1948.467300	11842.425216	62.317044
1947.464367	11789.256920	62.322049
1947.078070	11728.407198	62.327054
1946.410873	11663.778108	62.332058
1945.572816	11610.362938	62.337063
1945.388887	11547.825579	62.342068
1944.128846	11487.232301	62.347073
1943.981323	11428.655842	62.352078
1943.052398	11374.174140	62.357082
1942.309650	11305.817692	62.362087
1941.847550	11244.101770	62.367092
1941.066145	11182.678232	62.372097
1940.602464	11132.698007	62.377102
1939.845240	11070.740459	62.382106
1939.340654	11004.962030	62.387111
1938.565530	10944.001035	62.392116
1937.792540	10891.015598	62.397121
1937.309123	10815.576983	62.402126
1936.350437	10768.924542	62.407130
1935.596806	10707.162016	62.412135
1935.581849	10639.398043	62.417140
1934.550874	10599.623971	62.422145
1934.036257	10525.431687	62.427150
1933.348120	10475.836432	62.432154
1932.477588	10413.886159	62.437159
1932.255992	10349.965181	62.442164
1931.070488	10284.896831	62.447169
1930.787132	10224.333886	62.452174
1929.708287	10166.303472	62.457178
1928.985942	10100.751731	62.462183
1928.916005	10042.251178	62.467188
1928.249341	9998.739884	62.472193
1927.707854	9924.234504	62.477198
1926.886390	9867.640953	62.482202
1926.103845	9804.350994	62.487207
1925.923528	9738.257190	62.492212
1924.903045	9676.480903	62.497217
1924.040992	9608.615797	62.502222
1923.543388	9553.512460	62.507226
1923.155673	9483.103987	62.512231
1922.444320	9425.220865	62.517236
1921.274835	9364.016655	62.522241
1920.483757	9290.064885	62.527246
1919.742020	9257.709472	62.532250
1919.336922	9188.770988	62.537255
1918.721443	9127.510175	62.542260
1918.180149	9080.774243	62.547265
1917.970231	9020.977246	62.552270
1916.932364	8960.127747	62.557274
1916.276942	8895.321705	62.562279
1915.575913	8824.964877	62.567284
1914.844778	8779.074974	62.572289
1914.394206	8710.625569	62.577294
1913.457216	8650.645290	62.582298
1912.957669	8592.328636	62.587303
1912.231799	8522.930957	62.592308
1911.117302	8463.162635	62.597313
1910.471368	8417.000380	62.602318
1910.286304	8356.273169	62.607322
1909.108135	8302.794384	62.612327
1908.773153	8230.324431	62.617332
1907.818692	8190.657042	62.622337
1907.664064	8127.991587	62.627342
1906.665448	8079.339074	62.632346
1906.277281	8012.810184	62.637351
1905.947194	7939.779186	62.642356
1904.719535	7894.157398	62.647361
1904.232066	7833.146630	62.652366
1903.537444	7778.068095	62.657370
1902.937871	7714.597009	62.662375
1902.394080	7649.352278	62.667380
1901.540769	7590.245711	62.672385
1901.217263	7532.769437	62.677390
1900.248865	7481.952641	62.682394
1899.744820	7410.624991	62.687399
1898.994892	7357.889395	62.692404
1898.139721	7296.657583	62.697409
1897.590927	7247.734442	62.702414
1897.126002	7191.175685	62.707418
1896.259620	7138.242428	62.712423
1895.747185	7061.611348	62.717428
1895.003725	7005.952598	62.722433
1894.546861	6942.172656	62.727438
1893.619455	6890.283321	62.732442
1892.995620	6830.055576	62.737447
1892.593407	6776.788823	62.742452
1891.422177	6714.906761	62.747457
1891.270299	6652.466362	62.752462
1890.496458	6593.738448	62.757466
1889.560967	6525.530668	62.762471
1889.533673	6470.892150	62.767476
1888.364209	6421.304352	62.772481
1887.843534	6358.453621	62.777486
1887.088545	6292.964017	62.782490
1886.299281	6243.337755	62.787495
1886.148810	6186.239130	62.792500
1884.935430	6126.730970	62.797505
1884.604826	6055.819274	62.802510
1883.930626	6009.147613	62.807514
1882.883623	5940.785125	62.812519
1882.527992	5872.969440	62.817524
1881.636272	5824.366519	62.822529
1881.213080	5749.450695	62.827534
1880.659739	5709.394207	62.832538
1879.558276	5645.218170	62.837543
1879.138237	5586.061855	62.842548
1878.356152	5536.204937	62.847553
1877.518966	5484.009650	62.852558
1876.938282	5426.939662	62.857562
1876.445823	5381.118207	62.862567
1875.896214	5318.021729	62.867572
1875.043850	5270.188919	62.872577
1874.659342	5193.916314	62.877582
1873.921924	5147.949912	62.882586
1873.324709	5091.695440	62.887591
1872.749810	5029.621657	62.892596
1871.571064	4968.827859	62.897601
1871.139188	4907.123086	62.902606
1870.496701	4856.045105	62.907610
1869.874990	4794.016816	62.912615
1869.306589	4732.072602	62.917620
1868.148172	4701.473620	62.922625
1867.915174	4629.521656	62.927630
1867.145169	4581.988754	62.932634
1866.279809	4520.348903	62.937639
1866.005198	4461.699274	62.942644
1865.268982	4418.339987	62.947649
1864.596578	4354.797076	62.952654
1863.760185	4293.450909	62.957658
1863.239612	4237.442276	62.962663
1862.568591	4182.392315	62.967668
1861.789279	4130.352743	62.972673
1861.284645	4063.889259	62.977678
1860.712118	4016.341032	62.982682
1859.476194	3962.122139	62.987687
1859.507141	3898.862281	62.992692
1858.746015	3848.525892	62.997697
1857.999666	3786.999564	63.002702
1857.081901	3745.156116	63.007706
1856.550036	3680.179770	63.012711
1856.130713	3630.009106	63.017716
1854.978799	3578.539324	63.022721
1854.403575	3511.489398	63.027726
1853.894843	3463.716748	63.032730
1853.103815	3411.475758	63.037735
1852.715097	3358.480242	63.042740
1851.914518	3293.980439	63.047745
1851.195931	3245.174817	63.052750
1850.297236	3190.056692	63.057754
1850.088629	3133.439672	63.062759
1849.323439	3086.235767	63.067764
1848.431053	3031.526527	63.072769
1847.773102	2965.498498	63.077774
1847.304455	2932.896331	63.082778
1846.708599	2872.287602	63.087783
1845.820317	2829.420863	63.092788
1844.881259	2773.955060	63.097793
1844.723164	2711.085205	63.102798
1843.815986	2668.887508	63.107802
1842.604136	2608.283838	63.112807
1842.131031	2550.751361	63.117812
1841.443158	2522.026890	63.122817
1841.271744	2466.909577	63.127822
1840.495402	2419.893338	63.132826
1839.909509	2362.891294	63.137831
1839.451753	2308.235622	63.142836
1838.715056	2258.373186	63.147841
1838.308352	2196.634815	63.152846
1837.366053	2151.757562	63.157850
1836.644152	2099.392009	63.162855
1836.130311	2035.841877	63.167860
1835.218319	1999.163611	63.172865
1834.634970	1940.830950	63.177870
1833.836371	1897.752424	63.182874
1833.255770	1844.594155	63.187879
1832.578916	1791.161179	63.192884
1831.708586	1739.271535	63.197889
1831.349432	1688.838556	63.202894
1830.516765	1645.181884	63.207898
1830.162833	1594.925032	63.212903
1829.541391	1530.306021	63.217908
1828.557042	1478.356561	63.222913
1827.920109	1429.758534	63.227918
1827.143757	1379.148430	63.232922
1826.298707	1328.803313	63.237927
1825.916790	1281.797517	63.242932
1825.232303	1239.367543	63.247937
1824.898423	1185.486505	63.252942
1823.848092	1144.035877	63.257946
1822.951457	1095.410818	63.262951
1822.540616	1045.615137	63.267956
1821.884538	1008.040069	63.272961
1821.349385	950.140560	63.277966
1820.507407	913.227629	63.282970
1819.747615	859.353927	63.287975
1819.170674	808.827694	63.292980
1818.336155	769.960073	63.297985
1817.938576	723.718671	63.302990
1817.094147	681.227420	63.307994
1816.479767	632.115974	63.312999
1815.792625	585.701795	63.318004
1814.480391	543.305730	63.323009
1814.249617	502.967865	63.328014
1813.642748	471.093331	63.333018
1812.830688	410.062420	63.338023
1812.185598	377.672197	63.343028
1811.494173	334.052245	63.348033
1811.114356	301.339379	63.353038
1810.041245	263.487121	63.358042
1808.919569	235.821641	63.363047
1808.982311	192.777782	63.368052
1808.098416	148.625997	63.373057
1807.554914	118.383736	63.378062
1806.423849	87.570965	63.383066
1805.903867	54.027815	63.388071
1805.222079	24.452659	63.393076
1804.148759	-3.065503	63.398081
1803.601952	-38.843355	63.403086
1802.556110	-60.108700	63.408090
1801.359504	-69.879858	63.413095
1800.277464	-79.787468	63.418100
1795.663167	23.319661	63.423105
1795.476113	43.598190	63.428110
1796.122678	35.935884	63.433114
1796.873181	47.332724	63.438119
1797.748082	31.871126	63.443124
1797.028966	39.644252	63.448129
1795.505509	32.867407	63.453134
1794.487543	38.453536	63.458138
1794.157467	26.797520	63.463143
1794.011734	30.469564	63.468148
1792.616760	41.652022	63.473153
1792.209167	40.540365	63.478158
1791.353026	32.823380	63.483162
1790.215148	39.882445	63.488167
1789.691512	34.969987	63.493172
1789.360456	48.435571	63.498177
1789.282652	46.156681	63.503182
1788.623798	41.628378	63.508186
1787.870636	45.116196	63.513191
1787.516225	36.789702	63.518196
1786.362318	47.050828	63.523201
1785.708261	30.302440	63.528206
1785.030154	43.782132	63.533210
1784.031007	48.939519	63.538215
1783.914060	40.710928	63.543220
1782.855994	48.134203	63.548225
1781.955120	47.370527	63.553230
1781.164465	43.079189	63.558234
1781.492116	49.262165	63.563239
1781.263055	48.063813	63.568244
1779.617893	56.890720	63.573249
1779.077167	51.828014	63.578254
1778.594410	45.327440	63.583258
1777.732916	41.495190	63.588263
1777.525776	45.005108	63.593268
1776.586657	50.033122	63.598273
1775.785386	50.064153	63.603278
1775.722283	50.383224	63.608282
1774.244328	45.243859	63.613287
1774.092664	34.316418	63.618292
1773.294740	51.050923	63.623297
1772.263151	48.310087	63.628302
1772.197721	49.050557	63.633306
1771.717668	50.918118	63.638311
1770.526754	43.487680	63.643316
1769.510001	46.266762	63.648321
1769.653009	45.042440	63.653326
1768.784480	53.818556	63.658330
1767.871967	53.424149	63.663335
1767.386928	47.953650	63.668340
1766.837756	48.922322	63.673345
1765.929268	43.071234	63.678350
1765.399292	50.386998	63.683354
1764.802842	51.533484	63.688359
1763.985340	50.157355	63.693364
1763.426722	61.730551	63.698369
1762.828630	55.432789	63.703374
1762.256172	51.937826	63.708378
1761.721686	51.816112	63.713383
1761.000844	43.837961	63.718388
1759.820520	58.408211	63.723393
1759.320606	43.202771	63.728398
1759.014001	47.070671	63.733402
1758.462584	55.840584	63.738407
1758.114561	47.893107	63.743412
1757.391619	52.448422	63.748417
1756.811699	45.378257	63.753422
1755.619671	51.633841	63.758426
1754.099690	52.699921	63.763431
1754.390526	51.180896	63.768436
1753.134677	67.169738	63.773441
1752.948379	52.825930	63.778446
1752.419971	41.061067	63.783450
1751.660977	50.571967	63.788455
1751.114443	47.637418	63.793460
1750.084301	49.165006	63.798465
1749.643627	51.757995	63.803470
1749.339967	40.632350	63.808474
1748.394817	44.518084	63.813479
1748.179637	40.389245	63.818484
1747.314459	49.879163	63.823489
1747.044623	45.301705	63.828494
1745.599842	43.173682	63.833498
1744.617094	45.032776	63.838503
1744.352307	42.755201	63.843508
1743.153746	59.690536	63.848513
1742.810428	47.158291	63.853518
1742.901042	38.286487	63.858522
1741.903776	49.744842	63.863527
1741.412076	40.834634	63.868532
1740.698384	39.580794	63.873537
1740.169965	35.361362	63.878542
1739.688483	46.395617	63.883546
1738.501819	51.578069	63.888551
1737.401391	39.200766	63.893556
1736.531341	43.125036	63.898561
1736.539654	47.726638	63.903566
1736.163452	46.520120	63.908570
1735.035687	50.116330	63.913575
1734.617167	40.959545	63.918580
1733.675515	44.045244	63.923585
1733.374916	39.516828	63.928590
1733.205198	51.042446	63.933594
1732.046704	57.740553	63.938599
1731.377357	55.229196	63.943604
1730.327560	50.099125	63.948609
1729.594763	39.357020	63.953614
1729.039049	49.218822	63.958618
1728.195819	54.833996	63.963623
1728.249490	52.840145	63.968628
1727.442594	59.327878	63.973633
1726.871964	50.174747	63.978638
1726.485348	53.604368	63.983642
1725.647598	60.257845	63.988647
1725.003159	46.147655	63.993652
1723.436661	51.097137	63.998657
1723.136515	52.751638	64.003662
1722.715438	45.660987	64.008666
1721.835401	59.262653	64.013671
1721.508129	52.319520	64.018676
1720.921644	56.045803	64.023681
1720.616958	59.615371	64.028686
1719.976280	52.267870	64.033690
1718.652508	55.456842	64.038695
1718.075964	54.698445	64.043700
1717.096014	55.095327	64.048705
1716.846329	53.621147	64.053710
1716.574435	55.357890	64.058714
1716.133560	54.065457	64.063719
1714.922322	45.219073	64.068724
1713.627132	57.358670	64.073729
1713.013246	52.950971	64.078734
1712.450577	51.084972	64.083738
1711.632985	53.414568	64.088743
1711.725542	36.601238	64.093748
1711.091943	57.726526	64.098753
1710.679463	45.120124	64.103758
1709.996189	45.227048	64.108762
1709.365300	50.455276	64.113767
1708.370755	50.073919	64.118772
1707.442893	47.439634	64.123777
1706.994275	41.149692	64.128782
1706.732598	51.660205	64.133786
1705.489211	53.756245	64.138791
1704.525738	43.609004	64.143796
1703.810500	52.436478	64.148801
1703.870390	48.461066	64.153806
1703.090498	50.893482	64.158810
1702.220770	50.924370	64.163815
1702.020762	44.416753	64.168820
1701.333684	58.427727	64.173825
1700.528763	55.322925	64.178830
1699.333039	55.476553	64.183834
1698.753106	52.520513	64.188839
1698.501022	41.065003	64.193844
1697.814489	53.033814	64.198849
1697.192091	50.448782	64.203854
1697.020485	49.369041	64.208858
1695.610528	58.615934	64.213863
1694.724846	51.832460	64.218868
1694.024377	52.643836	64.223873
1693.482919	52.297748	64.228878
1693.194597	51.041011	64.233882
1692.395568	52.744792	64.238887
1692.361536	48.205579	64.243892
1691.416578	54.865052	64.248897
1690.503784	47.584437	64.253902
1690.028742	54.705415	64.258906
1689.320752	43.965690	64.263911
1688.751940	46.583770	64.268916
1687.565591	52.560945	64.273921
1686.629732	46.103979	64.278926
1686.181911	43.677295	64.283930
1685.444146	53.859746	64.288935
1685.213353	45.586173	64.293940
1684.250671	52.464496	64.298945
1684.212188	49.081851	64.303950
1683.985202	44.360407	64.308954
1682.868955	64.056437	64.313959
1682.156789	54.731842	64.318964
1681.415855	56.082637	64.323969
1680.953045	50.305865	64.328974
1679.485681	54.236724	64.333978
1678.662002	53.657934	64.338983
1678.934876	48.683635	64.343988
1678.107349	47.108863	64.348993
1677.525636	50.708243	64.353998
1676.940226	49.978072	64.359002
1675.999089	58.456675	64.364007
1675.111952	44.750895	64.369012
1674.310089	57.736203	64.374017
1673.965459	51.179022	64.379022
1673.320944	48.728391	64.384026
1672.660468	47.485040	64.389031
1672.469366	50.527233	64.394036
1671.267536	55.328939	64.399041
1670.306311	47.102007	64.404046
1669.547065	48.966626	64.409050
1669.141732	58.635827	64.414055
1668.745603	41.941120	64.419060
1668.399287	70.253985	64.424065
1668.088621	57.593567	64.429070
1667.041835	55.454407	64.434074
1665.911670	55.452562	64.439079
1665.734369	57.470740	64.444084
1664.984485	52.020257	64.449089
1663.793916	50.413273	64.454094
1663.041741	57.143054	64.459098
1662.193327	58.791614	64.464103
1661.744865	48.761271	64.469108
1661.188725	57.807902	64.474113
1660.716361	45.496445	64.479118
1660.475797	41.532492	64.484122
1659.769848	50.285960	64.489127
1659.356998	37.853097	64.494132
1658.250714	41.505844	64.499137
1657.692864	48.818164	64.504142
1657.152637	45.578297	64.509146
1655.999911	43.243091	64.514151
1655.358060	39.364960	64.519156
1654.460102	49.706895	64.524161
1654.051823	44.033428	64.529166
1654.063196	44.608742	64.534170
1653.206922	46.449355	64.539175
1652.776657	39.320761	64.544180
1651.477165	46.422897	64.549185
1650.552737	43.505825	64.554190
1650.276688	41.794577	64.559194
1649.739735	55.371715	64.564199
1649.309423	49.570866	64.569204
1648.053276	52.522056	64.574209
1647.173152	42.743210	64.579214
1646.669673	48.463699	64.584218
1646.516682	49.699032	64.589223
1646.297830	42.060634	64.594228
1644.788366	37.058817	64.599233
1644.039519	50.076700	64.604238
1643.592666	51.358713	64.609242
1643.100170	42.940648	64.614247
1642.599669	47.276156	64.619252
1641.624485	54.292091	64.624257
1640.888287	51.895455	64.629262
1640.529985	43.826642	64.634266
1639.589502	51.685430	64.639271
1639.293432	38.742032	64.644276
1638.283325	45.307790	64.649281
1637.228507	52.571332	64.654286
1636.475197	46.334538	64.659290
1635.926686	50.182531	64.664295
1635.999602	48.160393	64.669300
1634.961133	52.409481	64.674305
1634.940820	51.321479	64.679310
1634.393386	42.371271	64.684314
1633.171788	47.814770	64.689319
1632.574273	43.355614	64.694324
1631.541661	43.735663	64.699329
1631.035075	43.073402	64.704334
1630.157777	39.729400	64.709338
1629.525557	47.515566	64.714343
1628.995717	36.153082	64.719348
1628.178640	55.823664	64.724353
1628.132782	51.844551	64.729358
1627.773080	46.568633	64.734362
1626.829293	43.419690	64.739367
1626.069652	42.515367	64.744372
1625.191456	49.892774	64.749377
1624.792693	45.452505	64.754382
1623.754989	38.735794	64.759386
1622.839592	46.625290	64.764391
1622.562010	46.699326	64.769396
1622.192025	37.780857	64.774401
1621.779877	36.250500	64.779406
1620.707207	47.780785	64.784410
1619.650864	38.931929	64.789415
1619.508913	33.418007	64.794420
1618.416025	46.429047	64.799425
1617.901923	50.397728	64.804430
1617.006144	48.485326	64.809434
1616.030053	43.487098	64.814439
1616.173742	43.478442	64.819444
1615.589668	50.424366	64.824449
1614.973947	43.243242	64.829454
1613.884244	40.308289	64.834458
1613.129443	39.005826	64.839463
1612.498426	37.015097	64.844468
1612.072001	44.123624	64.849473
1611.670756	39.155497	64.854478
1610.716754	39.234496	64.859482
1609.740569	38.169045	64.864487
1609.670878	45.479509	64.869492
1608.905040	42.310188	64.874497
1608.276128	49.573882	64.879502
1607.110611	42.401261	64.884506
1606.322670	44.809751	64.889511
1606.210211	38.706118	64.894516
1605.871972	42.588515	64.899521
1605.006664	38.078875	64.904526
1604.014086	36.460966	64.909530
1603.109343	38.955818	64.914535
1602.977927	34.887806	64.919540
1602.294379	44.897655	64.924545
1601.256337	41.429396	64.929550
1600.292684	32.650981	64.934554
1599.888404	39.782795	64.939559
1599.565739	33.125957	64.944564
1599.053849	43.778712	64.949569
1598.466229	41.306449	64.954574
1597.311026	36.631565	64.959578
1596.616497	39.113522	64.964583
1596.519963	34.342985	64.969588
1595.667299	43.042501	64.974593
1594.705863	42.755272	64.979598
1594.071722	41.279110	64.984602
1593.229657	49.458151	64.989607
1592.946522	40.656771	64.994612
1592.489430	50.871912	64.999617
1591.568844	37.138380	65.004622
1590.865574	42.977344	65.009626
1589.854762	46.173422	65.014631
1589.968408	45.092523	65.019636
1588.843284	49.569850	65.024641
1588.060995	31.777520	65.029646
1587.711983	39.635383	65.034650
1586.850207	49.186295	65.039655
1586.697614	38.746291	65.044660
1585.431446	42.836035	65.049665
1584.877763	41.168904	65.054670
1584.373659	40.725446	65.059674
1583.700777	43.401078	65.064679
1583.116583	29.010166	65.069684
1581.979249	37.795909	65.074689
1581.090296	37.065102	65.079694
1580.815277	39.587641	65.084698
1580.055688	47.053443	65.089703
1580.234285	41.266254	65.094708
1579.366479	44.507421	65.099713
1578.133869	44.400470	65.104718
1577.414567	49.185472	65.109722
1576.858916	46.823247	65.114727
1576.700141	36.458342	65.119732
1575.965850	43.484902	65.124737
1575.172368	52.692245	65.129742
1574.623811	30.286660	65.134746
1573.612164	49.821001	65.139751
1573.143758	36.933386	65.144756
1571.973890	49.210804	65.149761
1571.192399	44.008220	65.154766
1570.896343	39.338767	65.159770
1570.088870	47.446086	65.164775
1570.165731	41.257186	65.169780
1569.384791	48.267508	65.174785
1568.527726	46.506662	65.179790
1567.521227	48.379055	65.184794
1566.861042	48.695227	65.189799
1566.643967	50.968876	65.194804
1565.929290	50.077927	65.199809
1564.776371	46.074447	65.204814
1564.168238	30.222416	65.209818
1563.486834	51.542941	65.214823
1563.303548	41.104661	65.219828
1562.711325	47.077370	65.224833
1562.111725	40.650610	65.229838
1561.299778	43.201692	65.234842
1560.689747	40.797652	65.239847
1560.265251	52.048362	65.244852
1558.804549	50.284083	65.249857
1557.838026	43.196561	65.254862
1557.767053	46.900886	65.259866
1557.268468	47.552493	65.264871
1557.111765	44.012028	65.269876
1556.058138	47.913481	65.274881
1555.224496	39.333613	65.279886
1554.542055	49.879438	65.284890
1554.256840	48.073468	65.289895
1553.239250	38.981955	65.294900
1552.103462	38.347145	65.299905
1551.460418	40.106604	65.304910
1551.039737	41.274090	65.309914
1550.556980	40.317912	65.314919
1550.384530	43.893287	65.319924
1549.153762	40.143449	65.324929
1548.331780	38.779143	65.329934
1548.035458	41.412298	65.334938
1547.173309	40.727705	65.339943
1547.476937	32.828125	65.344948
1546.270526	48.676696	65.349953
1545.288870	39.212063	65.354958
1545.019595	43.066161	65.359962
1543.639605	41.489333	65.364967
1542.996859	42.234808	65.369972
1542.405343	37.339504	65.374977
1542.149727	42.844010	65.379982
1541.702915	40.213777	65.384986
1540.809725	50.014108	65.389991
1539.707397	41.647241	65.394996
1538.846359	39.358780	65.400001
1538.651064	49.649016	65.405006
1538.448193	32.329171	65.410010
1537.787779	44.990829	65.415015
1537.157731	40.808094	65.420020
1536.107652	38.322600	65.425025
1535.794863	39.884513	65.430030
1534.623419	44.474871	65.435034
1533.263776	46.349774	65.440039
1533.089256	43.786658	65.445044
1532.561030	42.329951	65.450049
1532.266528	50.321081	65.455054
1532.118022	35.643344	65.460058
1530.975701	44.548166	65.465063
1530.021291	44.840139	65.470068
1529.410229	40.484086	65.475073
1529.044716	48.125391	65.480078
1528.171520	49.467282	65.485082
1526.966886	40.541114	65.490087
1527.027184	35.217407	65.495092
1526.089902	51.165142	65.500097
1525.863351	37.493245	65.505102
1524.845985	39.545566	65.510106
1523.901034	46.042664	65.515111
1523.632070	50.108019	65.520116
1523.202418	47.624866	65.525121
1522.368384	39.937591	65.530126
1521.811447	44.201661	65.535130
1520.956896	40.937660	65.540135
1520.825160	44.918134	65.545140
1519.247826	45.551933	65.550145
1518.242107	43.057821	65.555150
1518.150191	40.060553	65.560154
1517.424931	49.998202	65.565159
1517.327318	35.780716	65.570164
1516.444877	46.279480	65.575169
1515.306246	37.380678	65.580174
1514.916519	35.238099	65.585178
1514.458239	45.773538	65.590183
1514.366059	36.356809	65.595188
1512.583590	45.804887	65.600193
1512.007932	38.790890	65.605198
1511.720431	44.303618	65.610202
1511.043968	48.592992	65.615207
1510.710074	35.072192	65.620212
1509.607047	43.636478	65.625217
1509.063764	44.659457	65.630222
1508.492005	47.888294	65.635226
1507.367817	41.396682	65.640231
1506.739176	31.570061	65.645236
1505.960419	45.113085	65.650241
1505.796847	37.180513	65.655246
1505.486394	40.270060	65.660250
1504.515340	48.056473	65.665255
1503.755297	36.364774	65.670260
1502.941034	52.866954	65.675265
1502.762490	35.368215	65.680270
1502.133078	36.046928	65.685274
1500.657422	49.181903	65.690279
1500.177714	44.492760	65.695284
1499.423752	45.333186	65.700289
1499.400623	39.239022	65.705294
1498.876756	43.157234	65.710298
1497.698442	43.120538	65.715303
1497.416360	36.744264	65.720308
1496.640784	47.407393	65.725313
1495.781758	44.956208	65.730318
1494.992216	42.678478	65.735322
1493.771494	44.299522	65.740327
1493.804369	35.846901	65.745332
1493.288575	43.691852	65.750337
1492.552666	38.325943	65.755342
1491.880921	45.531809	65.760346
1490.863319	45.836992	65.765351
1490.795088	36.132621	65.770356
1490.338015	43.097800	65.775361
1489.141970	39.023945	65.780366
1488.856482	38.455883	65.785370
1488.144950	40.226239	65.790375
1487.066421	39.853583	65.795380
1486.210499	34.028953	65.800385
1485.642284	50.637106	65.805390
1485.429135	34.129426	65.810394
1484.740439	45.981913	65.815399
1484.467754	30.371486	65.820404
1482.857357	47.613587	65.825409
1482.250241	39.455048	65.830414
1482.161031	41.077627	65.835418
1481.442292	48.238926	65.840423
1480.579668	30.915137	65.845428
1479.782003	39.214871	65.850433
1479.502007	34.697417	65.855438
1478.904367	40.111203	65.860442
1477.658623	35.826066	65.865447
1477.173317	39.739729	65.870452
1476.404168	34.631410	65.875457
1476.164801	34.303591	65.880462
1475.717734	39.824331	65.885466
1474.989897	39.734980	65.890471
1474.442853	31.155335	65.895476
1473.654328	44.885988	65.900481
1472.806598	36.078169	65.905486
1471.789642	40.577771	65.910490
1471.170128	43.836280	65.915495
1470.887874	37.184083	65.920500
1470.092925	40.213440	65.925505
1469.042528	35.257047	65.930510
1468.945939	41.870063	65.935514
1467.895921	36.353816	65.940519
1467.788645	38.075456	65.945524
1466.762199	38.405707	65.950529
1465.916365	42.293092	65.955534
1465.765052	23.301470	65.960538
1464.893916	40.109133	65.965543
1464.148621	32.450360	65.970548
1463.197854	34.739691	65.975553
1462.425989	33.864167	65.980558
1462.276631	33.001674	65.985562
1461.555044	44.632319	65.990567
1460.738768	37.888380	65.995572
1459.919568	36.823269	66.000577
1459.419346	36.145840	66.005582
1459.128191	38.675683	66.010586
1458.255559	40.449573	66.015591
1457.426762	24.181673	66.020596
1456.661929	40.606606	66.025601
1456.341766	38.109221	66.030606
1455.918268	32.818251	66.035610
1454.748939	38.322895	66.040615
1454.323779	29.356473	66.045620
1453.667054	47.568189	66.050625
1452.986631	35.341909	66.055630
1452.436982	32.702809	66.060634
1451.046596	48.269999	66.065639
1450.903218	34.023533	66.070644
1450.609870	41.763752	66.075649
1449.310567	39.645896	66.080654
1448.612736	30.265513	66.085658
1447.759525	46.737615	66.090663
1447.755168	31.437774	66.095668
1447.136238	31.491965	66.100673
1446.382269	47.041587	66.105678
1445.895530	33.450485	66.110682
1444.716845	37.136896	66.115687
1444.794403	32.892192	66.120692
1443.528673	32.691226	66.125697
1442.688965	43.011333	66.130702
1442.491413	31.498338	66.135706
1441.642038	38.492753	66.140711
1441.504248	36.877825	66.145716
1440.284232	40.621268	66.150721
1439.646707	32.940645	66.155726
1439.480806	34.237959	66.160730
1437.732569	32.333379	66.165735
1436.862219	29.612794	66.170740
1436.645657	37.615186	66.175745
1436.532397	34.179789	66.180750
1436.318052	27.663460	66.185754
1435.373575	33.731590	66.190759
1434.653025	35.320474	66.195764
1433.782927	32.248204	66.200769
1433.276595	37.251688	66.205774
1432.574937	27.592812	66.210778
1431.188154	37.381727	66.215783
1430.874895	40.632568	66.220788
1430.259167	35.331156	66.225793
1429.906107	35.653741	66.230798
1429.963548	38.937125	66.235802
1428.821090	40.637219	66.240807
1428.298169	40.423854	66.245812
1427.218398	39.537357	66.250817
1426.063994	36.433008	66.255822
1425.564461	35.515790	66.260826
1425.038166	38.573419	66.265831
1424.702742	36.993057	66.270836
1423.575007	47.447254	66.275841
1422.932233	48.457679	66.280846
1422.701085	44.495416	66.285850
1421.911312	44.438000	66.290855
1421.370718	36.945393	66.295860
1420.411109	38.196978	66.300865
1419.679928	33.696054	66.305870
1419.582396	33.728880	66.310874
1418.332883	47.121245	66.315879
1417.441166	41.624012	66.320884
1417.361675	42.841365	66.325889
1416.817803	44.681282	66.330894
1416.494718	44.272162	66.335898
1415.288050	47.963036	66.340903
1414.520812	38.002360	66.345908
1413.996219	52.183067	66.350913
1413.064083	51.558526	66.355918
1412.117412	30.195538	66.360922
1411.239818	37.454631	66.365927
1411.099226	38.891421	66.370932
1410.728374	56.326039	66.375937
1410.280319	40.104857	66.380942
1409.937067	42.381223	66.385946
1408.658916	47.225125	66.390951
1408.377186	45.554232	66.395956
1407.526033	40.681310	66.400961
1406.356135	40.227021	66.405966
1405.982280	44.253863	66.410970
1405.197857	48.634532	66.415975
1405.238361	48.430963	66.420980
1404.072785	51.993891	66.425985
1403.093667	42.074778	66.430990
1402.889627	41.101136	66.435994
1402.063917	44.217399	66.440999
1401.313940	36.729695	66.446004
1400.565556	41.711736	66.451009
1400.101065	47.345638	66.456014
1400.024182	35.947504	66.461018
1398.842046	48.551764	66.466023
1397.907169	42.938402	66.471028
1397.524524	46.063087	66.476033
1396.864612	42.230477	66.481038
1395.690746	36.767064	66.486042
1394.847229	42.757664	66.491047
1394.753254	27.511504	66.496052
1393.969975	33.971898	66.501057
1393.803695	36.548127	66.506062
1393.220021	38.712905	66.511066
1392.082869	43.988544	66.516071
1391.554281	31.498473	66.521076
1391.304560	39.022032	66.526081
1390.084320	40.676162	66.531086
1389.801376	29.744430	66.536090
1388.676736	40.276985	66.541095
1388.088545	28.865518	66.546100
1387.352190	31.843006	66.551105
1386.384527	35.119024	66.556110
1385.992708	32.358663	66.561114
1385.698704	33.859260	66.566119
1385.355870	34.353683	66.571124
1384.429105	38.900477	66.576129
1383.741982	34.867203	66.581134
1383.348953	32.092842	66.586138
1381.911138	34.420196	66.591143
1381.608550	24.768868	66.596148
1380.794700	30.560795	66.601153
1380.699786	31.627642	66.606158
1379.741737	30.322866	66.611162
1378.859150	37.399843	66.616167
1378.315513	27.338995	66.621172
1377.648918	30.672810	66.626177
1376.368480	35.715774	66.631182
1375.773329	33.071309	66.636186
1374.953054	30.057371	66.641191
1374.704630	23.887077	66.646196
1374.714611	35.212215	66.651201
1373.949669	30.793941	66.656206
1373.140876	29.610516	66.661210
1372.386085	37.712654	66.666215
1372.138736	42.313874	66.671220
1371.106633	36.796402	66.676225
1370.124277	37.717321	66.681230
1369.787931	20.384062	66.686234
1369.112028	29.208483	66.691239
1368.384411	25.296766	66.696244
1367.798772	39.895579	66.701249
1366.891593	44.070276	66.706254
1366.672231	28.590173	66.711258
1365.286705	36.231202	66.716263
1364.958474	26.449918	66.721268
1364.164252	38.591991	66.726273
1363.523960	31.301324	66.731278
1363.785891	30.209463	66.736282
1362.682201	32.245605	66.741287
1362.010422	41.069379	66.746292
1361.384640	34.736727	66.751297
1360.558096	38.253661	66.756302
1359.776820	35.774399	66.761306
1359.052311	40.241744	66.766311
1358.729715	30.620405	66.771316
1357.585937	38.927876	66.776321
1356.887092	35.509882	66.781326
1356.434273	29.875104	66.786330
1355.889816	44.737024	66.791335
1355.803287	35.603259	66.796340
1354.757553	35.433594	66.801345
1353.927831	36.390178	66.806350
1353.337371	39.177335	66.811354
1351.965151	26.859233	66.816359
1351.565377	33.821620	66.821364
1351.014092	37.991783	66.826369
1350.569667	34.539654	66.831374
1350.181851	22.150224	66.836378
1348.893546	35.780570	66.841383
1347.954932	28.288185	66.846388
1347.644503	30.633452	66.851393
1347.215423	20.057690	66.856398
1347.166344	26.683642	66.861402
1345.963108	38.479170	66.866407
1344.985577	35.458702	66.871412
1344.523983	32.026650	66.876417
1344.145896	29.087503	66.881422
1343.619987	30.788965	66.886426
1342.542869	39.896364	66.891431
1342.361477	39.439498	66.896436
1341.403889	37.839787	66.901441
1340.683343	35.827095	66.906446
1340.317830	33.677544	66.911450
1339.511488	47.048368	66.916455
1338.590277	33.111651	66.921460
1337.495887	36.850935	66.926465
1336.649561	36.480852	66.931470
1336.826157	43.173432	66.936474
1336.071183	51.851177	66.941479
1335.850487	31.654831	66.946484
1334.639876	39.905130	66.951489
1334.177375	34.183591	66.956494
1333.418140	31.990980	66.961498
1332.042070	38.818429	66.966503
1331.899349	31.830278	66.971508
1331.379233	26.684002	66.976513
1330.824266	40.270315	66.981518
1330.672284	39.263174	66.986522
1329.398497	37.983380	66.991527
1328.996829	32.425629	66.996532
1328.036128	45.595499	67.001537
1326.935481	39.116006	67.006542
1326.761315	30.220097	67.011546
1325.850608	38.287110	67.016551
1325.594765	37.298057	67.021556
1325.106486	45.280573	67.026561
1324.062109	47.124385	67.031566
1323.864451	36.656902	67.036570
1322.769597	45.612595	67.041575
1322.455416	35.143137	67.046580
1321.279417	41.306456	67.051585
1320.545637	44.018637	67.056590
1320.286135	40.535538	67.061594
1319.688273	30.595286	67.066599
1319.272500	33.442982	67.071604
1318.245938	46.148684	67.076609
1317.374231	39.812564	67.081614
1316.329618	35.287389	67.086618
1315.741780	37.443383	67.091623
1315.288730	33.604720	67.096628
1315.108906	41.974993	67.101633
1314.599220	28.556316	67.106638
1313.968892	26.961356	67.111642
1312.586844	41.281528	67.116647
1312.321788	49.332634	67.121652
1311.879833	36.753122	67.126657
1310.677755	50.355595	67.131662
1310.484748	34.109676	67.136666
1309.846483	42.092384	67.141671
1309.214456	33.193577	67.146676
1307.853952	41.578099	67.151681
1307.376780	40.878113	67.156686
1306.890621	33.976103	67.161690
1306.484386	39.774208	67.166695
1305.945828	37.939166	67.171700
1304.972228	31.251840	67.176705
1304.251847	34.233118	67.181710
1303.926828	34.675836	67.186714
1302.743688	33.935130	67.191719
1302.001079	23.538530	67.196724
1301.743431	44.553572	67.201729
1301.107914	31.708387	67.206734
1300.529379	27.918062	67.211738
1299.590740	43.883393	67.216743
1299.324664	32.458589	67.221748
1298.754271	41.737742	67.226753
1297.470320	40.202549	67.231758
1296.995193	41.413421	67.236762
1296.340604	35.202058	67.241767
1296.100330	36.101215	67.246772
1294.685701	51.744857	67.251777
1294.101750	26.471953	67.256782
1293.663346	29.040989	67.261786
1293.263709	36.049089	67.266791
1292.556389	47.825721	67.271796
1291.550877	40.083806	67.276801
1290.931847	33.299115	67.281806
1290.732604	44.507709	67.286810
1290.097789	43.064849	67.291815
1289.088237	25.988444	67.296820
1288.257643	51.779499	67.301825
1287.962007	37.487889	67.306830
1287.630887	25.556217	67.311834
1286.319161	35.295414	67.316839
1285.687448	41.569321	67.321844
1285.142640	44.992602	67.326849
1284.220138	43.475639	67.331854
1283.866892	40.310211	67.336858
1283.094875	39.325962	67.341863
1282.922252	29.415881	67.346868
1281.948008	39.434148	67.351873
1280.612497	30.174136	67.356878
1280.123752	31.051300	67.361882
1279.561543	36.719671	67.366887
1279.267184	30.432120	67.371892
1278.884726	37.484798	67.376897
1277.915090	33.751929	67.381902
1277.293827	41.590019	67.386906
1276.377481	43.831367	67.391911
1276.290563	32.270855	67.396916
1275.200931	38.838332	67.401921
1274.920712	39.007438	67.406926
1274.420468	36.899818	67.411930
1273.257063	40.082424	67.416935
1272.270459	37.348844	67.421940
1271.801665	37.765542	67.426945
1271.650241	38.488155	67.431950
1270.678964	32.364999	67.436954
1269.478608	45.757482	67.441959
1269.389189	36.135354	67.446964
1268.732371	34.740151	67.451969
1267.865785	45.890855	67.456974
1267.198744	37.702493	67.461978
1266.298911	43.511279	67.466983
1265.961675	31.638924	67.471988
1265.793546	39.723498	67.476993
1265.063891	47.157799	67.481998
1264.173825	38.809365	67.487002
1263.533667	55.553544	67.492007
1262.802756	36.427044	67.497012
1261.827315	37.946119	67.502017
1261.198940	42.428163	67.507022
1260.925283	39.508692	67.512026
1260.238110	41.440807	67.517031
1259.189228	35.993860	67.522036
1258.588541	40.028398	67.527041
1257.953933	36.019928	67.532046
1257.882059	28.309350	67.537050
1256.526353	40.097616	67.542055
1256.110610	32.660899	67.547060
1255.489231	41.441985	67.552065
1255.062273	43.572412	67.557070
1254.341874	41.403611	67.562074
1253.395153	47.795419	67.567079
1253.107323	39.130469	67.572084
1252.047286	44.475899	67.577089
1251.168099	40.203557	67.582094
1250.779008	40.705353	67.587098
1250.204104	44.738947	67.592103
1250.065479	36.010854	67.597108
1248.780994	48.975196	67.602113
1247.872006	43.450818	67.607118
1247.868656	34.705947	67.612122
1246.358611	45.211527	67.617127
1245.471872	33.863346	67.622132
1245.199548	37.640679	67.627137
1244.823893	41.956392	67.632142
1244.528808	38.739147	67.637146
1243.927146	40.634015	67.642151
1243.335680	44.419520	67.647156
1242.685460	33.215075	67.652161
1241.800883	38.439571	67.657166
1240.762322	43.571864	67.662170
1240.034555	35.344286	67.667175
1239.572698	44.609343	67.672180
1239.145686	48.755037	67.677185
1238.234603	43.406030	67.682190
1237.669898	32.683129	67.687194
1236.937494	43.270056	67.692199
1236.329325	33.405583	67.697204
1235.364302	45.426615	67.702209
1234.643372	38.027390	67.707214
1234.239612	30.491008	67.712218
1233.671296	47.551746	67.717223
1233.222801	31.652391	67.722228
1232.355074	34.343316	67.727233
1231.494007	37.477864	67.732238
1231.583178	33.414235	67.737242
1230.114050	39.769272	67.742247
1229.621233	30.991854	67.747252
1228.785529	33.485309	67.752257
1228.126559	46.168851	67.757262
1228.402382	39.733871	67.762266
1226.755259	47.157958	67.767271
1226.260053	35.827947	67.772276
1225.976226	37.899349	67.777281
1225.064472	38.034848	67.782286
1224.475645	34.228833	67.787290
1223.474047	39.268525	67.792295
1223.104613	35.487545	67.797300
1222.589199	41.795007	67.802305
1221.523116	51.085191	67.807310
1220.965221	37.578014	67.812314
1220.416105	46.677185	67.817319
1220.168872	47.178505	67.822324
1219.147202	44.297564	67.827329
1218.303857	44.228230	67.832334
1218.070862	36.779806	67.837338
1217.033080	34.193154	67.842343
1216.534303	36.994142	67.847348
1215.552539	42.401250	67.852353
1215.066791	43.419870	67.857358
1214.899907	34.234250	67.862362
1213.483292	37.430338	67.867367
1212.817166	35.686562	67.872372
1212.473170	36.116541	67.877377
1212.044738	37.588072	67.882382
1211.558219	41.650193	67.887386
1210.601814	36.543362	67.892391
1209.957009	35.322875	67.897396
1209.595749	35.304611	67.902401
1208.441525	30.976681	67.907406
1207.621970	34.576122	67.912410
1207.252241	35.019654	67.917415
1206.860656	34.536302	67.922420
1205.736327	39.417329	67.927425
1204.876641	45.043138	67.932430
1204.807166	36.220481	67.937434
1204.287082	39.184124	67.942439
1203.537064	37.113085	67.947444
1202.803519	39.180315	67.952449
1201.926306	36.110839	67.957454
1201.298695	38.609057	67.962458
1200.168050	44.464028	67.967463
1199.587217	40.469098	67.972468
1199.240384	48.342407	67.977473
1198.768543	50.658168	67.982478
1198.011413	28.462539	67.987482
1197.128520	34.664443	67.992487
1196.820037	38.286689	67.997492
1196.371798	36.419963	68.002497
1195.050722	38.120178	68.007502
1194.541262	33.708643	68.012506
1193.854533	39.803665	68.017511
1193.917972	30.750151	68.022516
1192.920323	28.904568	68.027521
1191.816100	40.011077	68.032526
1191.518630	34.391055	68.037530
1190.882917	30.671350	68.042535
1189.832911	25.875871	68.047540
1188.930180	36.221817	68.052545
1188.751974	30.625407	68.057550
1188.441960	27.312780	68.062554
1187.615565	38.980629	68.067559
1186.551069	32.041319	68.072564
1185.962003	30.706324	68.077569
1185.380667	43.656630	68.082574
1185.184278	24.771595	68.087578
1183.730980	25.838436	68.092583
1183.597029	40.460043	68.097588
1183.044015	32.791296	68.102593
1182.028250	35.616162	68.107598
1181.210641	31.554820	68.112602
1180.567264	47.564681	68.117607
1180.238349	27.741975	68.122612
1180.030149	29.239984	68.127617
1178.859486	35.345740	68.132622
1178.700995	27.746713	68.137626
1177.640032	32.887318	68.142631
1176.806126	29.423054	68.147636
1176.072404	28.879006	68.152641
1175.268166	39.266062	68.157646
1174.896734	41.185830	68.162650
1173.638328	37.353855	68.167655
1173.265534	27.727929	68.172660
1172.616830	32.063417	68.177665
1172.155923	34.039989	68.182670
1172.321391	33.132177	68.187674
1171.051369	35.179082	68.192679
1170.140424	32.785157	68.197684
1169.628845	39.150359	68.202689
1169.426417	35.639283	68.207694
1168.494250	15.294400	68.212698
1167.509204	36.712086	68.217703
1167.055447	30.976583	68.222708
1165.904366	36.662934	68.227713
1165.442094	32.079907	68.232718
1164.934707	26.551622	68.237722
1164.465607	33.555010	68.242727
1163.513787	31.900837	68.247732
1162.371534	29.825964	68.252737
1162.124796	35.303839	68.257742
1161.761162	27.316414	68.262746
1161.187297	31.575350	68.267751
1161.137564	28.763779	68.272756
1160.097678	43.631962	68.277761
1159.133546	33.451984	68.282766
1158.212418	32.994514	68.287770
1157.013126	42.540854	68.292775
1156.527086	36.272769	68.297780
1156.612015	36.708651	68.302785
1156.202512	40.700188	68.307790
1155.166901	38.010719	68.312794
1154.041356	34.238046	68.317799
1153.576522	37.309600	68.322804
1153.472631	35.506384	68.327809
1152.564725	39.203466	68.332814
1151.571682	37.022869	68.337818
1151.189933	35.490914	68.342823
1150.462239	35.922003	68.347828
1149.771522	31.685957	68.352833
1148.839623	34.650454	68.357838
1148.686800	29.035820	68.362842
1148.053540	38.605672	68.367847
1147.281154	19.541040	68.372852
1146.333484	29.102546	68.377857
1146.022028	35.546303	68.382862
1145.391354	22.038128	68.387866
1143.929931	37.293458	68.392871
1143.593166	28.265754	68.397876
1143.160902	29.063000	68.402881
1142.681596	39.269080	68.407886
1142.149287	28.323454	68.412890
1140.993331	42.330203	68.417895
1140.897044	24.690763	68.422900
1139.917256	35.963565	68.427905
1138.664335	31.115229	68.432910
1138.537324	33.426613	68.437914
1137.781645	31.198809	68.442919
1137.887022	35.900048	68.447924
1136.496271	33.282841	68.452929
1135.564234	41.542525	68.457934
1135.291181	34.997732	68.462938
1134.877110	37.963448	68.467943
1133.662865	42.634888	68.472948
1132.957187	30.264532	68.477953
1132.601828	35.223546	68.482958
1132.295669	26.883227	68.487962
1131.284221	45.389484	68.492967
1130.652333	33.206077	68.497972
1130.158715	28.046177	68.502977
1129.150195	37.190037	68.507982
1128.310946	24.949737	68.512986
1127.848353	40.222822	68.517991
1127.326040	30.303735	68.522996
1127.178450	37.210262	68.528001
1126.277152	30.539903	68.533006
1125.510732	27.369261	68.538010
1124.851399	33.921963	68.543015
1123.869877	27.581318	68.548020
1123.201510	36.699462	68.553025
1122.363941	39.289436	68.558030
1122.217454	28.449599	68.563034
1121.313754	34.747870	68.568039
1120.452902	33.661114	68.573044
1120.102884	38.617703	68.578049
1119.204696	31.018070	68.583054
1119.256473	19.173772	68.588058
1118.030311	29.121764	68.593063
1117.719967	38.925674	68.598068
1117.135445	25.588354	68.603073
1115.809488	35.840792	68.608078
1115.293985	31.755076	68.613082
1114.647764	32.742469	68.618087
1114.207520	37.727602	68.623092
1113.555365	27.300919	68.628097
1112.653503	41.415486	68.633102
1112.071590	20.447242	68.638106
1111.404641	38.636938	68.643111
1110.882420	29.911539	68.648116
1110.054187	29.603306	68.653121
1109.149974	37.418620	68.658126
1108.924868	30.675405	68.663130
1108.223480	36.741237	68.668135
1107.351376	39.221597	68.673140
1106.750868	34.091317	68.678145
1106.543238	29.327460	68.683150
1105.909488	33.748888	68.688154
1104.580004	39.613444	68.693159
1104.154949	33.384557	68.698164
1103.791643	37.507516	68.703169
1102.499747	37.168962	68.708174
1101.914561	33.597357	68.713178
1101.287014	40.402041	68.718183
1100.917933	32.259383	68.723188
1100.513281	21.110553	68.728193
1099.967190	43.667903	68.733198
1099.335149	40.597312	68.738202
1098.362437	39.124675	68.743207
1097.471559	28.087872	68.748212
1096.414204	32.423725	68.753217
1095.572689	41.859563	68.758222
1095.833302	26.530257	68.763226
1095.183739	41.997079	68.768231
1094.607467	41.046406	68.773236
1093.661595	36.064100	68.778241
1092.750794	26.812342	68.783246
1092.357929	34.331866	68.788250
1091.396166	41.082487	68.793255
1090.741411	39.090943	68.798260
1090.210663	26.090415	68.803265
1089.729330	32.841880	68.808270
1089.607049	27.436851	68.813274
1088.383857	35.140490	68.818279
1087.635725	41.688404	68.823284
1087.460821	39.951678	68.828289
1085.985458	37.062543	68.833294
1085.365227	34.748558	68.838298
1084.667999	34.075735	68.843303
1084.854466	31.493088	68.848308
1084.457296	38.147594	68.853313
1082.975361	38.463723	68.858318
1082.720193	28.480080	68.863322
1081.776291	34.862024	68.868327
1080.928795	30.614672	68.873332
1080.480601	21.216800	68.878337
1079.907210	32.693039	68.883342
1078.972319	36.582085	68.888346
1078.006023	29.316565	68.893351
1077.985957	31.692936	68.898356
1077.553661	24.194248	68.903361
1076.375323	29.030300	68.908366
1075.589712	30.008338	68.913370
1074.941090	26.260761	68.918375
1074.714548	26.727264	68.923380
1074.301793	30.449678	68.928385
1073.347139	30.331870	68.933390
1072.597892	33.746707	68.938394
1071.824343	30.703368	68.943399
1070.597100	37.983479	68.948404
1070.119222	35.896000	68.953409
1069.110890	28.727053	68.958414
1069.323959	30.328359	68.963418
1068.968680	36.651365	68.968423
1068.581687	39.084529	68.973428
1067.262057	29.331716	68.978433
1066.619202	41.638989	68.983438
1065.961302	29.754624	68.988442
1064.890433	35.767282	68.993447
1064.702028	31.651622	68.998452
1064.085866	31.358552	69.003457
1063.196684	31.697088	69.008462
1062.392063	22.639758	69.013466
1061.802853	35.318520	69.018471
1061.340358	19.243279	69.023476
1060.952196	35.229882	69.028481
1059.927667	34.774704	69.033486
1059.533275	32.383802	69.038490
1058.727330	23.509600	69.043495
1057.523291	34.762906	69.048500
1056.621030	32.724018	69.053505
1055.989507	34.738788	69.058510
1056.025543	34.348276	69.063514
1055.860401	32.102246	69.068519
1055.046773	26.245833	69.073524
1054.183217	27.417618	69.078529
1053.413470	24.955548	69.083534
1053.170633	26.670377	69.088538
1051.640635	39.733760	69.093543
1051.071461	38.818236	69.098548
1050.710523	32.765234	69.103553
1050.138923	37.386512	69.108558
1049.431602	34.968125	69.113562
1048.363350	29.174295	69.118567
1047.833887	40.446446	69.123572
1047.473445	39.836746	69.128577
1047.000041	28.620019	69.133582
1046.430411	30.279608	69.138586
1045.518651	37.181551	69.143591
1044.689345	32.917126	69.148596
1043.874845	39.612795	69.153601
1043.102772	31.490109	69.158606
1042.957900	34.411434	69.163610
1042.004668	26.907322	69.168615
1041.711305	35.349262	69.173620
1040.547754	37.413982	69.178625
1040.008450	32.113145	69.183630
1040.118057	23.485943	69.188634
1039.051954	38.039791	69.193639
1038.277871	32.385239	69.198644
1037.693728	31.979854	69.203649
1036.587068	23.317497	69.208654
1035.842311	29.508507	69.213658
1035.223154	25.295807	69.218663
1034.812212	35.106258	69.223668
1034.620259	29.630321	69.228673
1033.490336	29.671292	69.233678
1032.847866	30.508305	69.238682
1032.071649	31.232561	69.243687
1031.528471	33.088209	69.248692
1030.894242	30.106294	69.253697
1030.075359	33.057581	69.258702
1029.724257	19.604321	69.263706
1029.068033	27.706611	69.268711
1028.066382	36.841524	69.273716
1027.616018	26.671339	69.278721
1027.045765	36.816204	69.283726
1026.754788	28.708446	69.288730
1025.427861	34.337675	69.293735
1025.081991	23.483850	69.298740
1024.655900	30.330606	69.303745
1023.361657	33.447403	69.308750
1023.058267	26.852269	69.313754
1022.056843	25.819449	69.318759
1021.900248	32.320571	69.323764
1020.692468	27.480888	69.328769
1019.611784	29.739004	69.333774
1019.512903	23.592284	69.338778
1019.198105	33.059448	69.343783
1018.519922	32.476650	69.348788
1018.050892	40.129719	69.353793
1017.037452	35.106159	69.358798
1016.680673	27.217021	69.363802
1015.372419	30.660886	69.368807
1014.641575	33.252835	69.373812
1014.271470	30.730350	69.378817
1013.976959	24.310417	69.383822
1013.557820	28.711910	69.388826
1012.288704	21.731133	69.393831
1011.738599	26.785789	69.398836
1011.434395	15.900115	69.403841
1010.223125	28.849723	69.408846
1009.845187	23.997864	69.413850
1008.966204	32.906693	69.418855
1008.445012	24.458695	69.423860
1007.949451	21.063661	69.428865
1006.733598	30.495993	69.433870
1006.440129	31.794702	69.438874
1006.134079	21.871213	69.443879
1005.177412	26.143772	69.448884
1004.373506	23.324472	69.453889
1003.659348	35.952159	69.458894
1003.610655	16.204791	69.463898
1002.469980	26.128184	69.468903
1001.816277	26.899186	69.473908
1001.250492	18.693242	69.478913
1000.386468	34.068035	69.483918
999.993047	29.849390	69.488922
999.182508	24.147042	69.493927
998.973631	37.593159	69.498932
997.960677	28.341928	69.503937
996.674386	29.681909	69.508942
996.801149	14.788637	69.513946
996.130614	33.688497	69.518951
994.994077	25.694779	69.523956
994.738657	23.765879	69.528961
994.194056	29.240689	69.533966
993.409953	15.055283	69.538970
991.703634	31.161722	69.543975
991.677296	18.338013	69.548980
990.995784	20.535783	69.553985
990.520346	26.915752	69.558990
990.423872	19.626996	69.563994
989.207897	30.100092	69.568999
988.273673	29.592731	69.574004
988.048637	27.378314	69.579009
987.554877	23.837925	69.584014
987.181964	28.153222	69.589018
986.084415	26.087089	69.594023
985.335619	30.162587	69.599028
984.283818	26.780369	69.604033
983.532487	27.295686	69.609038
983.349179	21.192365	69.614042
982.833768	37.505128	69.619047
982.595707	24.141119	69.624052
981.239790	23.672472	69.629057
980.544318	28.562615	69.634062
980.483171	20.902404	69.639066
979.181255	20.213865	69.644071
978.417913	30.938207	69.649076
978.057420	24.505125	69.654081
977.594940	34.185014	69.659086
977.103880	11.163490	69.664090
975.754253	33.378762	69.669095
975.379855	28.870104	69.674100
975.236380	23.605650	69.679105
973.920311	29.606892	69.684110
973.184755	28.552289	69.689114
972.495805	25.476600	69.694119
972.106330	35.174835	69.699124
971.739763	13.874372	69.704129
970.753152	34.841348	69.709134
969.982981	17.671862	69.714138
969.672155	29.323940	69.719143
968.744637	25.657039	69.724148
967.975214	29.617558	69.729153
967.456669	33.464046	69.734158
966.997580	27.554408	69.739162
966.205074	30.667087	69.744167
965.458417	27.341976	69.749172
964.915319	33.803676	69.754177
964.398103	35.655206	69.759182
963.633999	32.211451	69.764186
962.855531	22.733706	69.769191
961.955621	21.175428	69.774196
961.893791	28.156607	69.779201
960.854582	25.124039	69.784206
960.295890	28.056021	69.789210
959.546480	25.861969	69.794215
958.913687	26.156591	69.799220
958.352823	33.627166	69.804225
957.276676	28.526886	69.809230
957.407040	16.157620	69.814234
956.156540	33.665927	69.819239
955.208701	28.184127	69.824244
954.826919	20.120799	69.829249
954.169051	34.964505	69.834254
953.833785	17.593368	69.839258
952.684699	24.209835	69.844263
952.249768	18.841958	69.849268
951.519190	21.544260	69.854273
951.307644	23.694066	69.859278
950.489560	15.039455	69.864282
949.453579	28.872624	69.869287
948.756204	30.095267	69.874292
948.739893	27.425039	69.879297
947.435266	20.803171	69.884302
946.825107	22.104971	69.889306
946.468059	37.763364	69.894311
946.043590	27.078174	69.899316
945.389092	17.727363	69.904321
944.286920	24.415212	69.909326
943.651090	22.622540	69.914330
942.381272	28.818277	69.919335
941.910104	27.131861	69.924340
941.690171	32.745819	69.929345
941.116889	27.631758	69.934350
940.844339	21.542643	69.939354
939.797039	26.690619	69.944359
938.955793	23.582408	69.949364
938.824522	22.124168	69.954369
937.804153	33.441323	69.959374
936.987180	20.754469	69.964378
936.378743	31.872041	69.969383
935.965211	33.081058	69.974388
935.317502	27.108407	69.979393
934.105388	32.473415	69.984398
933.813954	25.365489	69.989402
933.171026	28.227306	69.994407
932.343938	32.144974	69.999412
931.832334	22.593238	70.004417
930.678778	35.645653	70.009422
930.750827	20.172915	70.014426
929.952486	36.152250	70.019431
929.339667	28.012153	70.024436
928.256995	26.353666	70.029441
927.584084	33.913034	70.034446
927.688421	22.640681	70.039450
926.415883	33.182724	70.044455
925.651920	26.761821	70.049460
925.325620	30.506763	70.054465
925.046833	35.150850	70.059470
923.824841	21.030422	70.064474
922.979769	36.224027	70.069479
922.562826	26.602038	70.074484
922.282222	30.301864	70.079489
920.720406	41.908610	70.084494
920.050313	24.254883	70.089498
919.274799	37.860548	70.094503
919.270589	25.507962	70.099508
919.245978	29.244319	70.104513
918.289440	31.776018	70.109518
917.531999	26.659732	70.114522
916.843760	29.112468	70.119527
916.161415	36.228662	70.124532
915.433558	29.543409	70.129537
914.955894	32.899299	70.134542
913.864287	28.892697	70.139546
912.830729	35.768330	70.144551
912.760480	29.596563	70.149556
912.433879	37.550235	70.154561
910.991438	32.744797	70.159566
910.398155	29.723286	70.164570
909.884007	24.151992	70.169575
909.634217	35.554677	70.174580
909.189936	30.358596	70.179585
908.147597	37.005405	70.184590
907.517535	24.262010	70.189594
906.877961	41.993226	70.194599
905.555743	26.814902	70.199604
905.152865	29.315264	70.204609
904.840722	28.977006	70.209614
904.529342	25.013395	70.214618
903.520248	29.515093	70.219623
902.681764	32.445883	70.224628
902.233308	24.965580	70.229633
901.122519	31.651666	70.234638
900.341906	23.502015	70.239642
899.386693	34.108681	70.244647
899.091693	31.284119	70.249652
899.001552	29.324197	70.254657
898.550909	21.470526	70.259662
897.890254	19.328598	70.264666
896.867199	29.003088	70.269671
896.567746	35.403949	70.274676
895.770385	15.614910	70.279681
894.608148	34.872134	70.284686
894.363197	22.926855	70.289690
893.674235	27.888517	70.294695
892.476791	21.470385	70.299700
891.971916	27.889742	70.304705
891.226988	25.035866	70.309710
891.112101	24.760830	70.314714
890.093840	29.718132	70.319719
889.158211	24.346378	70.324724
888.810218	25.275326	70.329729
888.230810	38.430339	70.334734
888.139857	19.186435	70.339738
886.875242	30.633932	70.344743
886.155528	34.080385	70.349748
885.836676	24.214150	70.354753
884.712382	40.448787	70.359758
884.027848	30.129838	70.364762
883.306619	28.484808	70.369767
883.139759	24.222247	70.374772
882.693208	21.365040	70.379777
881.306108	34.459368	70.384782
881.008606	18.197094	70.389786
880.308064	25.986357	70.394791
879.626027	29.207629	70.399796
878.578244	24.686317	70.404801
878.140808	32.741201	70.409806
877.762482	17.923593	70.414810
877.381103	29.962195	70.419815
876.878303	27.148632	70.424820
875.826500	28.750960	70.429825
875.050695	34.532232	70.434830
874.178939	28.864903	70.439834
873.393570	38.037977	70.444839
873.122948	32.940416	70.449844
872.520297	22.136960	70.454849
871.420652	28.359257	70.459854
870.650339	33.267645	70.464858
870.174955	30.936973	70.469863
869.707236	31.815596	70.474868
869.375131	27.268691	70.479873
868.611652	32.953389	70.484878
867.838368	28.803112	70.489882
867.242960	40.402724	70.494887
866.536015	27.129134	70.499892
865.507633	37.821570	70.504897
865.052411	39.546564	70.509902
864.701590	23.862026	70.514906
863.654544	43.096205	70.519911
862.811739	31.955671	70.524916
862.392308	26.388236	70.529921
861.911082	36.659292	70.534926
861.835625	39.654727	70.539930
860.358735	34.768075	70.544935
859.619607	34.504087	70.549940
859.606442	27.085396	70.554945
858.452801	37.487125	70.559950
857.577514	27.455578	70.564954
856.769432	34.143963	70.569959
856.475934	27.949390	70.574964
856.332570	21.477048	70.579969
855.007717	38.210365	70.584974
854.945163	30.304395	70.589978
854.055334	29.993435	70.594983
852.955688	24.097472	70.599988
852.122372	27.079490	70.604993
851.987720	22.229941	70.609998
851.736644	29.564495	70.615002
850.480041	31.855409	70.620007
849.396688	40.826770	70.625012
849.270951	26.178685	70.630017
848.887188	38.244480	70.635022
848.253467	27.764503	70.640026
847.056591	28.505307	70.645031
846.249796	35.806893	70.650036
846.285222	22.675343	70.655041
845.441630	27.708933	70.660046
844.444226	31.215363	70.665050
843.908548	21.607566	70.670055
843.555479	26.700271	70.675060
842.760053	25.450243	70.680065
841.605418	33.871582	70.685070
841.633428	24.566706	70.690074
840.877301	35.397155	70.695079
839.982543	27.880675	70.700084
839.681554	24.449980	70.705089
838.551092	24.680348	70.710094
837.861675	28.290715	70.715098
836.457457	23.570703	70.720103
836.079682	24.149602	70.725108
836.096380	19.637069	70.730113
835.250148	32.470293	70.735118
835.265226	23.005060	70.740122
834.413422	25.769263	70.745127
833.358634	21.283780	70.750132
833.172915	27.172977	70.755137
832.127051	31.403024	70.760142
831.792142	21.370634	70.765146
830.913579	32.614788	70.770151
829.732573	24.357016	70.775156
829.111120	15.177598	70.780161
828.417950	34.423252	70.785166
828.504577	10.371607	70.790170
827.767889	27.660975	70.795175
827.193551	22.414659	70.800180
826.488573	20.062199	70.805185
825.428138	31.633330	70.810190
824.613998	20.631755	70.815194
823.667194	14.364572	70.820199
823.421667	19.541078	70.825204
823.254440	19.652826	70.830209
822.389693	29.797277	70.835214
821.519497	29.691352	70.840218
820.794689	25.334690	70.845223
820.306429	29.201610	70.850228
819.463843	19.376183	70.855233
818.426586	23.070303	70.860238
818.426446	20.613539	70.865242
817.861459	18.539981	70.870247
816.996492	31.540184	70.875252
816.107797	17.546541	70.880257
815.509468	27.740044	70.885262
815.167506	27.223627	70.890266
813.819486	32.760121	70.895271
813.058552	30.123272	70.900276
813.139223	18.786893	70.905281
812.055318	30.281343	70.910286
811.968077	22.782990	70.915290
811.190146	27.400882	70.920295
810.577648	27.003218	70.925300
809.985308	24.456223	70.930305
808.448092	19.260684	70.935310
808.078551	19.824085	70.940314
807.729937	35.586778	70.945319
807.022583	22.177673	70.950324
806.525460	18.565327	70.955329
804.944034	31.042521	70.960334
804.953626	20.012331	70.965338
804.538506	26.701249	70.970343
803.776240	21.226247	70.975348
802.966204	26.423232	70.980353
802.327913	28.134800	70.985358
801.669611	15.736554	70.990362
801.177843	21.321246	70.995367
800.399968	29.651088	71.000372
800.041431	12.342056	71.005377
799.047175	31.332875	71.010382
798.299660	22.067880	71.015386
797.481583	23.453271	71.020391
796.610863	24.385019	71.025396
796.514412	19.748581	71.030401
796.036508	30.272985	71.035406
795.512679	25.223630	71.040410
794.381293	28.648908	71.045415
793.700084	25.100558	71.050420
793.098305	12.284911	71.055425
792.188002	30.037138	71.060430
791.751923	17.940971	71.065434
791.236886	21.810580	71.070439
790.558999	35.466951	71.075444
789.859771	24.693088	71.080449
789.162826	30.212680	71.085454
788.807230	22.069532	71.090458
787.572513	30.344373	71.095463
786.870628	23.620343	71.100468
786.327735	15.421863	71.105473
785.723021	31.786685	71.110478
785.834516	19.387321	71.115482
784.349133	39.738330	71.120487
783.792015	29.660898	71.125492
783.581099	29.401154	71.130497
782.277193	35.214479	71.135502
781.719139	15.463097	71.140506
780.966958	26.989899	71.145511
780.504125	28.336090	71.150516
780.225870	23.984047	71.155521
779.050233	40.351458	71.160526
778.531335	24.230102	71.165530
777.955557	23.952751	71.170535
777.282923	30.983849	71.175540
776.078949	32.326604	71.180545
775.519766	34.069739	71.185550
775.493806	18.905924	71.190554
775.013377	28.430994	71.195559
773.767056	23.629117	71.200564
773.454200	23.596902	71.205569
772.353212	26.902238	71.210574
772.608349	10.328115	71.215578
771.422317	35.142893	71.220583
770.776534	16.348450	71.225588
770.600394	17.723117	71.230593
769.357325	22.862895	71.235598
768.826494	18.708750	71.240602
768.143953	29.713564	71.245607
767.063656	21.477641	71.250612
766.395546	16.801331	71.255617
765.508567	26.630806	71.260622
765.368022	19.738580	71.265626
765.042181	23.369927	71.270631
764.164254	29.367744	71.275636
763.543332	12.444252	71.280641
762.556746	30.088786	71.285646
762.405195	20.134451	71.290650
761.244171	24.466430	71.295655
760.631185	25.152167	71.300660
760.305637	18.484926	71.305665
759.630652	31.680389	71.310670
758.785081	19.554808	71.315674
758.061185	26.666604	71.320679
757.540487	24.500859	71.325684
756.789942	11.543338	71.330689
755.594694	24.618204	71.335694
755.178756	15.502283	71.340698
754.961431	28.721075	71.345703
754.563200	19.924015	71.350708
753.484388	23.175367	71.355713
752.849068	29.377402	71.360718
752.598071	22.059660	71.365722
751.620068	26.819799	71.370727
750.381281	25.736573	71.375732
750.124534	25.903576	71.380737
749.462269	18.668656	71.385742
749.044172	22.721524	71.390746
748.453993	22.247787	71.395751
747.788367	28.752676	71.400756
747.212805	23.411965	71.405761
745.727832	28.976600	71.410766
745.157631	27.864204	71.415770
744.707837	26.913979	71.420775
744.070812	25.891065	71.425780
743.913393	32.263011	71.430785
742.784003	34.554224	71.435790
742.551740	27.255574	71.440794
742.069080	31.701904	71.445799
740.788819	34.373509	71.450804
740.338211	19.873363	71.455809
739.173161	28.126093	71.460814
739.309062	16.937040	71.465818
738.226950	27.843052	71.470823
737.589046	19.561946	71.475828
737.231044	25.142697	71.480833
736.177170	29.064988	71.485838
735.681759	23.257381	71.490842
734.581054	31.536138	71.495847
734.089445	31.078248	71.500852
733.937184	35.822044	71.505857
732.843195	27.777541	71.510862
732.369209	26.534718	71.515866
731.439807	25.728658	71.520871
731.590851	26.125614	71.525876
730.836612	21.453564	71.530881
729.276751	35.903185	71.535886
729.209335	13.255847	71.540890
728.611781	26.554092	71.545895
727.396675	26.919406	71.550900
727.194793	13.105033	71.555905
726.545420	32.149762	71.560910
726.061540	21.261221	71.565914
724.883430	23.583849	71.570919
724.332686	26.431035	71.575924
724.065847	23.461675	71.580929
722.635831	36.192337	71.585934
722.131652	20.308349	71.590938
721.649978	22.136918	71.595943
721.071619	37.240788	71.600948
721.040460	17.642074	71.605953
719.695005	37.983441	71.610958
719.253743	26.701780	71.615962
718.446500	22.266820	71.620967
717.859863	32.665048	71.625972
716.968890	23.123319	71.630977
716.203657	26.599137	71.635982
716.044807	21.619421	71.640986
715.269491	23.111564	71.645991
714.396563	17.092850	71.650996
713.885101	23.391858	71.656001
713.009150	26.901073	71.661006
713.004230	15.654023	71.666010
711.611271	30.386139	71.671015
710.896397	22.978266	71.676020
710.721339	19.130171	71.681025
710.072721	39.617626	71.686030
709.095949	15.844116	71.691034
708.565070	29.393511	71.696039
707.871518	26.704970	71.701044
707.669663	20.297151	71.706049
706.217316	39.991682	71.711054
705.731794	23.068722	71.716058
705.504489	23.158505	71.721063
704.745653	30.607020	71.726068
704.075177	22.586563	71.731073
703.258324	35.317371	71.736078
702.770557	24.279652	71.741082
701.910639	27.038881	71.746087
701.008505	25.935193	71.751092
700.720935	28.548104	71.756097
700.231605	28.526651	71.761102
699.513957	27.879265	71.766106
698.426277	23.036402	71.771111
697.777743	18.819019	71.776116
697.584337	25.530989	71.781121
696.455611	38.503836	71.786126
695.617127	31.047840	71.791130
695.277802	35.630620	71.796135
695.012338	25.732275	71.801140
694.497153	20.519155	71.806145
692.710332	34.170764	71.811150
692.542304	23.406974	71.816154
692.170409	14.454360	71.821159
691.603899	30.292736	71.826164
690.998792	23.220612	71.831169
689.921351	23.934588	71.836174
689.712243	27.323441	71.841178
688.808423	35.066269	71.846183
687.988668	23.969457	71.851188
687.348648	24.192762	71.856193
686.760676	31.883721	71.861198
686.485450	14.605612	71.866202
685.417484	31.848404	71.871207
684.732368	31.358261	71.876212
684.378125	27.756306	71.881217
683.102074	24.881416	71.886222
682.793731	18.329717	71.891226
682.271179	28.049149	71.896231
681.559925	32.659613	71.901236
680.608113	30.578298	71.906241
679.613356	28.219986	71.911246
679.604833	15.037119	71.916250
678.915630	23.251945	71.921255
678.199681	26.369860	71.926260
677.372085	22.319758	71.931265
676.776577	22.998001	71.936270
676.333424	18.498777	71.941274
676.130177	34.001786	71.946279
674.791832	26.983343	71.951284
674.718126	23.781399	71.956289
673.313699	35.525617	71.961294
672.515542	27.607496	71.966298
671.959568	28.839234	71.971303
671.353366	32.193552	71.976308
671.475169	31.169670	71.981313
670.632656	37.453598	71.986318
669.435269	25.330462	71.991322
668.758888	31.457054	71.996327
668.410641	29.932462	72.001332
667.588753	32.121127	72.006337
666.711851	35.061260	72.011342
666.490093	25.613255	72.016346
665.795425	34.811349	72.021351
665.038723	31.967305	72.026356
664.447704	28.392018	72.031361
664.051229	35.841189	72.036366
663.142867	30.998170	72.041370
662.240112	37.395766	72.046375
661.423330	30.674305	72.051380
661.172491	36.942863	72.056385
659.865972	36.181112	72.061390
659.150752	30.949390	72.066394
658.563664	31.321960	72.071399
658.351721	34.148325	72.076404
658.257719	22.257908	72.081409
657.620198	33.704980	72.086414
656.519671	27.883368	72.091418
655.840244	28.861969	72.096423
654.878881	27.967992	72.101428
654.245017	28.966145	72.106433
653.333849	30.940386	72.111438
653.278848	24.073973	72.116442
652.890578	29.003575	72.121447
651.622057	26.269421	72.126452
651.094408	22.934771	72.131457
650.242189	40.419178	72.136462
650.089169	26.727909	72.141466
648.940607	28.440348	72.146471
648.299396	25.817604	72.151476
648.168055	19.966239	72.156481
646.878219	37.268030	72.161486
646.079216	24.709328	72.166490
645.324582	33.694635	72.171495
645.204663	20.403358	72.176500
645.107667	19.228247	72.181505
644.060940	31.905788	72.186510
643.303452	21.809856	72.191514
642.692936	22.033205	72.196519
641.655387	28.229930	72.201524
641.015939	35.318846	72.206529
640.687736	33.119319	72.211534
640.462832	28.504924	72.216538
639.041419	33.241102	72.221543
638.084147	28.796947	72.226548
637.994147	26.892208	72.231553
637.252660	24.654423	72.236558
636.674493	20.285511	72.241562
635.497381	29.680277	72.246567
635.289124	26.975975	72.251572
635.143179	27.246763	72.256577
633.972437	34.406095	72.261582
633.316709	28.001179	72.266586
632.697860	35.988786	72.271591
632.171589	20.817941	72.276596
631.159503	25.537818	72.281601
629.948769	29.245445	72.286606
629.675768	26.037395	72.291610
629.412670	33.711319	72.296615
629.006189	36.753159	72.301620
628.365315	31.301462	72.306625
627.363993	33.315298	72.311630
627.017852	27.529677	72.316634
625.866444	22.758495	72.321639
625.110822	32.179179	72.326644
624.869018	24.861572	72.331649
623.990132	29.997034	72.336654
623.497225	18.562792	72.341658
622.714524	27.123662	72.346663
622.457787	23.947715	72.351668
621.773426	12.941338	72.356673
620.240905	27.318841	72.361678
620.090718	29.111984	72.366682
619.442939	28.023011	72.371687
618.565861	21.845731	72.376692
618.059087	25.289875	72.381697
617.360130	31.502071	72.386702
616.860440	22.987693	72.391706
616.036008	25.812256	72.396711
615.050650	24.731316	72.401716
614.697484	19.777828	72.406721
614.316179	19.251936	72.411726
613.782392	22.976334	72.416730
612.900544	31.477309	72.421735
611.808515	28.128474	72.426740
612.103639	15.849688	72.431745
610.943438	24.596827	72.436750
610.009453	20.916913	72.441754
609.765077	18.770272	72.446759
608.646478	26.138913	72.451764
607.603793	7.239043	72.456769
607.165159	12.263392	72.461774
606.685466	21.573901	72.466778
606.007724	24.078655	72.471783
606.064769	10.163156	72.476788
605.092471	17.751332	72.481793
604.338765	19.516018	72.486798
603.746648	16.779819	72.491802
602.837889	25.485341	72.496807
601.928847	18.606723	72.501812
601.830199	11.356210	72.506817
600.833574	34.899862	72.511822
600.036843	13.155569	72.516826
599.340085	19.876741	72.521831
599.078466	31.560403	72.526836
598.836022	14.193526	72.531841
597.462091	28.993614	72.536846
596.778590	21.809433	72.541850
596.131466	17.434170	72.546855
595.766228	30.848389	72.551860
595.089141	12.727612	72.556865
594.103782	19.275563	72.561870
593.799870	21.115266	72.566874
593.024246	17.982541	72.571879
592.112432	21.566886	72.576884
591.734046	9.322836	72.581889
591.131610	21.074961	72.586894
590.447472	23.530277	72.591898
589.536440	19.796256	72.596903
588.786043	20.376192	72.601908
588.431059	24.445836	72.606913
587.704841	24.137298	72.611918
586.900863	24.585427	72.616922
586.247033	20.586529	72.621927
585.549073	25.538652	72.626932
585.244682	24.435997	72.631937
584.571812	17.259590	72.636942
583.808931	17.081466	72.641946
583.193533	15.255680	72.646951
582.654091	35.128112	72.651956
581.869781	25.537919	72.656961
581.085973	28.750241	72.661966
580.600326	15.184510	72.666970
579.467095	21.678752	72.671975
578.641301	21.986863	72.676980
578.473973	14.086582	72.681985
577.840085	23.062127	72.686990
577.635953	19.174526	72.691994
576.893940	23.171778	72.696999
576.014656	20.762006	72.702004
575.489512	19.013304	72.707009
574.382384	20.525222	72.712014
573.841422	15.645806	72.717018
573.420278	21.443196	72.722023
572.137661	25.193833	72.727028
571.604082	26.392064	72.732033
570.911439	29.564639	72.737038
570.757758	21.947594	72.742042
570.132530	24.018239	72.747047
569.014865	25.544452	72.752052
568.557476	17.283538	72.757057
567.828644	22.332040	72.762062
567.422110	10.950294	72.767066
566.334160	20.468065	72.772071
565.694367	23.692143	72.777076
565.567083	16.748950	72.782081
564.618160	28.791224	72.787086
563.807825	20.600716	72.792090
563.507603	16.952337	72.797095
562.838498	15.327488	72.802100
561.837087	25.610452	72.807105
560.781105	28.650099	72.812110
560.496293	23.841844	72.817114
560.274926	22.699161	72.822119
559.401894	25.766436	72.827124
558.698889	28.718325	72.832129
557.933711	29.779993	72.837134
557.403909	17.949548	72.842138
556.320486	21.963339	72.847143
555.408778	23.302221	72.852148
555.310963	17.308340	72.857153
554.713234	32.028968	72.862158
554.407105	23.811767	72.867162
553.237869	27.292056	72.872167
552.566123	32.210054	72.877172
552.181769	13.165931	72.882177
551.643181	25.768863	72.887182
550.806345	25.821713	72.892186
549.808720	29.273093	72.897191
549.373596	41.583608	72.902196
549.095621	23.989016	72.907201
547.598432	26.742572	72.912206
547.050332	18.060896	72.917210
546.703235	23.896954	72.922215
546.319980	29.084374	72.927220
546.180084	20.336101	72.932225
544.804814	30.588742	72.937230
544.131827	28.827327	72.942234
543.380509	20.102331	72.947239
542.374421	26.606298	72.952244
542.219422	23.502461	72.957249
541.735371	29.909086	72.962254
540.951663	25.934042	72.967258
540.122444	24.402507	72.972263
539.523434	20.224590	72.977268
539.083249	16.849231	72.982273
538.250833	26.337350	72.987278
537.361031	18.077516	72.992282
536.845424	21.819530	72.997287
535.864527	32.110277	73.002292
535.120388	24.897931	73.007297
534.552172	27.065152	73.012302
534.438150	32.100886	73.017306
533.814434	27.209429	73.022311
532.930980	25.390084	73.027316
532.169696	18.311353	73.032321
531.135272	28.459246	73.037326
531.222368	21.936045	73.042330
530.044467	20.376481	73.047335
529.322098	22.107813	73.052340
528.834533	30.216439	73.057345
528.482614	42.198328	73.062350
527.913890	19.310785	73.067354
527.080234	23.392030	73.072359
526.428220	24.478256	73.077364
526.029090	24.243784	73.082369
524.811029	33.102673	73.087374
524.230035	26.367363	73.092378
523.720323	21.254336	73.097383
522.677350	25.977595	73.102388
521.832314	19.024166	73.107393
521.150209	23.863397	73.112398
521.161755	30.802905	73.117402
520.650021	36.160598	73.122407
519.936750	26.648997	73.127412
519.256470	21.348687	73.132417
518.870541	29.472661	73.137422
517.763771	23.764073	73.142426
516.770954	28.925600	73.147431
515.997748	28.966748	73.152436
515.998855	41.870060	73.157441
514.706005	26.242654	73.162446
514.268827	20.897313	73.167450
513.636982	26.004493	73.172455
512.734817	26.873540	73.177460
512.637793	23.424599	73.182465
511.803538	35.948492	73.187470
511.163166	30.591364	73.192474
510.606600	26.345195	73.197479
509.665054	19.178499	73.202484
508.947103	18.077081	73.207489
508.435051	33.840566	73.212494
508.131306	29.563584	73.217498
507.062031	21.367042	73.222503
506.170017	27.859157	73.227508
505.690291	16.826533	73.232513
505.443171	25.286342	73.237518
504.679812	15.434246	73.242522
503.614209	17.726434	73.247527
502.820417	19.518034	73.252532
502.854661	14.231635	73.257537
501.641204	25.054569	73.262542
501.197206	19.025959	73.267546
500.703714	17.794175	73.272551
499.929628	24.237545	73.277556
499.402169	25.220362	73.282561
498.670143	27.057314	73.287566
498.102521	19.938284	73.292570
497.013367	18.586937	73.297575
496.203945	19.491676	73.302580
496.192548	11.930824	73.307585
495.482100	26.664677	73.312590
494.876169	14.808539	73.317594
493.926210	15.631594	73.322599
492.925382	29.505010	73.327604
492.911029	17.803776	73.332609
491.542729	25.713681	73.337614
491.002200	23.152210	73.342618
490.542030	23.209727	73.347623
489.962969	29.782873	73.352628
489.399967	21.877829	73.357633
488.618341	23.836219	73.362638
487.955937	22.478391	73.367642
487.358678	22.161954	73.372647
486.250295	20.525109	73.377652
485.425845	19.672463	73.382657
484.924549	32.818215	73.387662
484.456915	13.432589	73.392666
484.266661	24.445744	73.397671
483.783031	18.218460	73.402676
482.846673	19.487181	73.407681
482.040776	27.495144	73.412686
481.650165	14.554517	73.417690
480.583490	24.906245	73.422695
479.742472	24.584491	73.427700
479.544914	14.659614	73.432705
478.962909	25.765140	73.437710
478.054032	21.152507	73.442714
477.265464	21.416876	73.447719
476.793755	25.486203	73.452724
476.380758	19.400624	73.457729
474.965058	23.047936	73.462734
474.707198	12.158165	73.467738
474.386062	9.724166	73.472743
473.406792	18.242267	73.477748
472.731146	25.981913	73.482753
472.139682	24.376257	73.487758
471.616034	16.058121	73.492762
470.784031	13.243487	73.497767
469.762168	22.313972	73.502772
469.519181	9.835508	73.507777
468.781699	16.493811	73.512782
468.262826	21.892066	73.517786
467.569081	25.083763	73.522791
466.513422	17.682968	73.527796
466.436887	12.789514	73.532801
465.540732	17.349061	73.537806
464.865101	12.815965	73.542810
464.245606	21.724582	73.547815
463.633706	24.054887	73.552820
462.880151	9.563689	73.557825
461.986983	30.563159	73.562830
461.614736	19.437734	73.567834
461.274371	19.100876	73.572839
460.035005	18.044698	73.577844
459.621403	20.343411	73.582849
458.890391	28.361526	73.587854
458.361704	22.833668	73.592858
457.813003	11.931894	73.597863
456.998979	31.250434	73.602868
456.285761	18.485780	73.607873
455.062012	32.000507	73.612878
454.671447	26.501104	73.617882
454.231734	20.374056	73.622887
453.495868	27.175605	73.627892
453.647138	18.136545	73.632897
451.986506	23.946928	73.637902
451.846393	27.994968	73.642906
451.372458	20.799527	73.647911
450.225642	21.223477	73.652916
449.276482	26.244037	73.657921
448.592213	18.919691	73.662926
448.626583	17.114992	73.667930
447.807230	22.434973	73.672935
446.642101	21.108368	73.677940
446.441138	27.499863	73.682945
446.044394	22.783572	73.687950
444.941829	23.933717	73.692954
443.926825	21.679651	73.697959
443.323524	30.817496	73.702964
443.208341	25.417716	73.707969
442.904605	22.585154	73.712974
441.867089	34.769304	73.717978
441.253446	23.893642	73.722983
440.370683	15.804609	73.727988
439.401400	12.031050	73.732993
438.571704	23.259615	73.737998
438.216035	19.121800	73.743002
438.279598	18.624401	73.748007
437.090784	23.769874	73.753012
436.508277	26.065542	73.758017
435.753061	22.943811	73.763022
435.412217	23.434887	73.768026
434.406552	15.758078	73.773031
433.397646	27.773672	73.778036
433.159763	12.588501	73.783041
432.383509	22.909740	73.788046
432.138658	29.363418	73.793050
431.155243	16.321723	73.798055
430.626643	31.755127	73.803060
430.301063	12.829411	73.808065
428.828234	29.928622	73.813070
428.289595	26.124295	73.818074
427.535205	23.052895	73.823079
427.262081	25.586260	73.828084
427.103796	22.743141	73.833089
425.831881	19.795198	73.838094
425.447719	23.186724	73.843098
424.701507	20.055679	73.848103
423.441014	34.296901	73.853108
422.930883	14.408742	73.858113
421.883246	31.085416	73.863118
422.176021	11.898765	73.868122
421.809177	21.066737	73.873127
420.566518	29.249955	73.878132
420.286891	5.967936	73.883137
419.519583	26.229879	73.888142
418.453682	20.161614	73.893146
418.107633	19.989661	73.898151
417.309887	26.083603	73.903156
416.775854	9.217383	73.908161
415.777845	19.692220	73.913166
415.439714	23.533704	73.918170
414.934619	20.676463	73.923175
414.196664	29.739578	73.928180
413.169223	17.149582	73.933185
412.717564	21.950542	73.938190
411.841269	19.117757	73.943194
410.974527	16.589362	73.948199
410.197934	25.155611	73.953204
410.027333	15.161801	73.958209
409.434118	21.555872	73.963214
409.231717	17.901393	73.968218
408.184629	22.833495	73.973223
407.579804	24.680165	73.978228
406.797848	20.482553	73.983233
405.833993	22.392737	73.988238
405.194814	30.774679	73.993242
405.150476	23.917630	73.998247
403.776290	33.495263	74.003252
403.213997	26.306028	74.008257
402.344788	27.600348	74.013262
402.401157	29.362164	74.018266
402.067252	23.159925	74.023271
400.775439	29.804079	74.028276
400.158786	22.550973	74.033281
399.521222	30.987849	74.038286
398.406090	24.692483	74.043290
397.876272	24.936147	74.048295
397.268657	24.928871	74.053300
397.107825	30.921334	74.058305
396.298451	21.600130	74.063310
395.793633	14.742347	74.068314
395.029713	21.469533	74.073319
394.147264	30.599828	74.078324
393.233473	17.089768	74.083329
392.290959	26.190210	74.088334
391.820410	25.265436	74.093338
391.779666	25.275061	74.098343
391.074995	23.476165	74.103348
390.521703	18.726489	74.108353
389.648946	26.753012	74.113358
389.144854	12.680962	74.118362
388.035592	21.003773	74.123367
387.397836	22.436249	74.128372
386.954052	21.587631	74.133377
386.370886	20.294471	74.138382
385.493174	26.025870	74.143386
385.086984	18.674582	74.148391
384.244596	25.035829	74.153396
383.950541	18.814630	74.158401
382.562719	21.085677	74.163406
382.155543	16.471984	74.168410
381.758827	19.389302	74.173415
381.140255	17.639765	74.178420
380.362845	25.247418	74.183425
379.448333	26.507966	74.188430
379.146016	25.439699	74.193434
378.308903	26.326812	74.198439
377.313747	26.762896	74.203444
376.710877	24.629256	74.208449
376.264530	27.720056	74.213454
376.007703	19.253779	74.218458
375.202441	22.354464	74.223463
374.352894	21.203098	74.228468
374.159269	26.480158	74.233473
372.850497	26.013793	74.238478
372.042656	33.050746	74.243482
372.079941	16.957616	74.248487
371.241831	29.264538	74.253492
370.429311	20.030575	74.258497
369.255117	27.319860	74.263502
368.835000	14.079634	74.268506
368.306168	20.392494	74.273511
367.998906	17.011758	74.278516
367.301531	16.652961	74.283521
366.580980	15.739647	74.288526
366.027896	21.901840	74.293530
364.948099	11.707591	74.298535
363.933515	26.969292	74.303540
363.814610	11.323659	74.308545
362.959596	23.488200	74.313550
362.522040	30.551298	74.318554
361.786521	24.059849	74.323559
360.959413	30.866498	74.328564
360.684604	16.477236	74.333569
360.053936	19.671521	74.338574
359.112552	18.804439	74.343578
358.764225	18.629704	74.348583
357.938224	25.018306	74.353588
356.988829	17.859240	74.358593
356.377410	21.438367	74.363598
355.537669	27.755048	74.368602
355.316592	21.771368	74.373607
354.616505	25.623233	74.378612
353.519900	22.585894	74.383617
353.093303	24.161336	74.388622
352.507573	28.209432	74.393626
352.494192	16.299916	74.398631
351.369296	26.631005	74.403636
350.988282	9.587469	74.408641
349.596410	32.049337	74.413646
348.818955	20.323080	74.418650
348.552130	14.786639	74.423655
347.866933	26.884703	74.428660
347.557544	15.728796	74.433665
346.745765	28.966607	74.438670
345.891453	19.319869	74.443674
345.630109	14.099505	74.448679
344.667212	34.914577	74.453684
343.772328	22.800203	74.458689
342.906438	30.726303	74.463694
342.313405	31.147201	74.468698
342.256636	12.408900	74.473703
341.535706	31.955455	74.478708
340.500726	21.810837	74.483713
340.088187	20.600878	74.488718
339.685690	28.776386	74.493722
338.791691	23.983254	74.498727
337.865051	29.296712	74.503732
337.793960	21.191904	74.508737
336.557094	18.098084	74.513742
335.733565	24.639254	74.518746
335.221607	11.733781	74.523751
334.682792	28.453955	74.528756
334.439516	19.260170	74.533761
333.468090	18.680144	74.538766
332.971174	24.814469	74.543770
332.554388	20.235431	74.548775
331.162742	22.967560	74.553780
330.967443	18.575562	74.558785
330.238188	20.080978	74.563790
329.194670	23.006771	74.568794
328.739449	16.415476	74.573799
327.609697	30.719466	74.578804
327.372373	21.136823	74.583809
326.818184	30.451351	74.588814
326.080978	18.210941	74.593818
325.212002	14.998576	74.598823
324.337605	26.158602	74.603828
324.155064	17.210593	74.608833
323.898474	15.922170	74.613838
322.716182	25.035615	74.618842
321.986608	16.023409	74.623847
321.268196	29.459221	74.628852
321.278055	20.471085	74.633857
320.362098	29.460091	74.638862
319.237930	21.882641	74.643866
319.249941	26.849401	74.648871
318.287604	17.587303	74.653876
317.454006	13.730674	74.658881
316.588863	26.934418	74.663886
316.138771	27.395615	74.668890
315.799871	19.257803	74.673895
314.817180	29.805925	74.678900
314.544960	16.562642	74.683905
313.761052	27.227307	74.688910
312.513966	20.282851	74.693914
311.968426	20.275164	74.698919
311.478698	24.248045	74.703924
310.931965	22.365659	74.708929
310.642634	22.764967	74.713934
309.729185	30.523624	74.718938
309.252278	22.461420	74.723943
308.434914	28.526980	74.728948
307.873972	13.760739	74.733953
306.795495	34.261519	74.738958
306.307167	20.155442	74.743962
306.103821	14.487474	74.748967
304.924228	33.277704	74.753972
304.322555	12.615757	74.758977
303.621324	14.920912	74.763982
302.847765	24.757652	74.768986
301.873774	24.726795	74.773991
301.241136	23.952445	74.778996
301.046875	22.975771	74.784001
300.863687	24.895604	74.789006
300.032395	25.089573	74.794010
298.889439	35.175996	74.799015
298.371297	28.170555	74.804020
297.901086	18.632923	74.809025
296.648950	26.947004	74.814030
296.332318	19.575156	74.819034
296.013642	20.218826	74.824039
295.581936	17.520219	74.829044
294.422329	23.384877	74.834049
293.583758	23.603660	74.839054
292.972351	16.542133	74.844058
292.707376	25.589805	74.849063
291.834021	17.051509	74.854068
291.440341	19.466913	74.859073
290.925168	23.991023	74.864078
289.356692	21.126690	74.869082
288.875454	23.428323	74.874087
287.792301	24.196995	74.879092
288.023048	19.872708	74.884097
287.259110	17.728497	74.889102
286.278874	22.416613	74.894106
285.947093	18.364902	74.899111
285.571326	19.484424	74.904116
285.192873	23.444303	74.909121
283.848224	22.116430	74.914126
283.313276	25.910453	74.919130
282.116819	18.921679	74.924135
281.040977	22.221629	74.929140
280.904192	19.036072	74.934145
280.193672	24.537438	74.939150
280.001260	30.640583	74.944154
279.879606	15.596187	74.949159
278.777665	31.420585	74.954164
278.157449	26.744679	74.959169
277.677699	31.770897	74.964174
276.547355	29.186801	74.969178
275.920741	28.075625	74.974183
275.185266	28.399401	74.979188
274.763461	14.490884	74.984193
273.567675	18.896411	74.989198
272.757857	31.074273	74.994202
272.803013	17.777260	74.999207
272.098784	23.648187	75.004212
271.957359	18.900700	75.009217
270.602184	14.056535	75.014222
269.852440	23.752299	75.019226
269.459755	24.757832	75.024231
268.129102	23.364663	75.029236
267.802757	14.833801	75.034241
267.210174	28.604357	75.039246
266.837859	28.263158	75.044250
266.657681	30.611421	75.049255
265.144567	32.812622	75.054260
264.793516	26.075433	75.059265
264.325310	27.206539	75.064270
263.383335	25.811339	75.069274
262.725946	22.251476	75.074279
262.181823	15.491453	75.079284
261.734731	22.753185	75.084289
260.591295	14.398296	75.089294
259.625085	32.553741	75.094298
259.359583	26.520389	75.099303
259.096734	23.843755	75.104308
258.079658	20.746480	75.109313
257.079612	27.505031	75.114318
256.686368	17.124137	75.119322
256.313204	18.112369	75.124327
255.248788	27.773145	75.129332
254.757166	20.183209	75.134337
254.270076	26.625044	75.139342
253.656164	23.636961	75.144346
253.256051	21.220314	75.149351
251.846988	20.877227	75.154356
251.342157	22.257011	75.159361
251.051632	24.662284	75.164366
250.324293	17.786398	75.169370
249.903995	17.698840	75.174375
249.143031	29.820036	75.179380
248.374516	16.517116	75.184385
247.288264	27.401866	75.189390
247.093819	14.532537	75.194394
245.650691	24.113341	75.199399
245.307013	16.118226	75.204404
244.688188	21.866741	75.209409
244.206052	22.088645	75.214414
243.815835	20.700114	75.219418
243.117975	12.237941	75.224423
242.000725	29.594342	75.229428
241.676850	17.420539	75.234433
241.260438	13.943690	75.239438
240.248137	29.630812	75.244442
239.540779	26.985615	75.249447
238.856501	28.706225	75.254452
238.547188	20.289340	75.259457
237.370106	18.975781	75.264462
236.482341	24.226305	75.269466
236.590975	11.829032	75.274471
235.839534	25.615450	75.279476
235.138009	16.625614	75.284481
234.122813	30.625958	75.289486
233.959512	16.072308	75.294490
233.306759	6.940670	75.299495
232.181172	17.391744	75.304500
231.693532	17.417420	75.309505
230.999112	28.421054	75.314510
230.251412	16.923486	75.319514
229.450304	13.845411	75.324519
228.930294	23.605479	75.329524
228.751993	18.272554	75.334529
227.920559	29.203418	75.339534
226.659082	20.720713	75.344538
226.214765	16.584456	75.349543
225.688657	23.314771	75.354548
225.363790	21.308733	75.359553
224.231698	23.283648	75.364558
223.559702	18.803662	75.369562
223.556636	15.875900	75.374567
222.549135	29.409846	75.379572
221.629832	15.008252	75.384577
221.060437	25.906804	75.389582
220.401895	19.500904	75.394586
220.296984	18.502108	75.399591
219.163702	18.659094	75.404596
218.493712	22.239703	75.409601
217.805899	18.421369	75.414606
216.554859	22.536127	75.419610
216.216247	15.584093	75.424615
215.623378	14.161645	75.429620
215.492432	15.751474	75.434625
214.567421	17.445814	75.439630
213.657756	20.474886	75.444634
213.084827	7.289037	75.449639
212.923598	24.045205	75.454644
212.478397	12.717032	75.459649
211.298170	18.979224	75.464654
210.569469	9.586904	75.469658
209.953073	16.815707	75.474663
208.694618	22.448590	75.479668
208.567086	13.961738	75.484673
207.935346	23.564589	75.489678
207.589486	22.713009	75.494682
206.366989	16.904768	75.499687
205.530824	15.555799	75.504692
205.549599	16.399559	75.509697
204.969287	15.683121	75.514702
203.996259	16.519423	75.519706
203.027374	17.232070	75.524711
202.298413	21.818659	75.529716
202.274286	12.712963	75.534721
201.244170	7.924248	75.539726
200.456618	23.892492	75.544730
200.188764	3.175814	75.549735
199.413157	13.342457	75.554740
198.476591	15.514856	75.559745
197.829077	14.687715	75.564750
197.291234	23.395711	75.569754
196.797231	17.286844	75.574759
196.087169	15.406872	75.579764
195.320322	6.194096	75.584769
194.370771	14.568777	75.589774
194.009354	15.228735	75.594778
193.773811	16.836818	75.599783
192.350777	11.598266	75.604788
192.331332	15.059398	75.609793
191.823991	18.131563	75.614798
190.621300	18.165595	75.619802
190.118929	11.258599	75.624807
189.600712	12.392960	75.629812
188.704415	20.000686	75.634817
187.924580	19.475324	75.639822
187.304762	12.391522	75.644826
186.975239	20.041346	75.649831
185.910700	13.534617	75.654836
185.024422	9.684861	75.659841
184.400731	25.690060	75.664846
183.776309	24.379875	75.669850
183.802502	10.292743	75.674855
183.023014	16.656627	75.679860
182.092563	14.654109	75.684865
181.555633	17.161747	75.689870
180.776662	16.620481	75.694874
180.458771	0.527260	75.699879
179.237076	24.600393	75.704884
178.664756	11.950589	75.709889
178.328786	18.344684	75.714894
177.713636	21.456116	75.719898
177.069922	21.169238	75.724903
176.232914	20.153130	75.729908
175.683960	13.889039	75.734913
174.208690	25.442923	75.739918
173.514979	3.889030	75.744922
173.378046	14.611404	75.749927
172.676448	18.526626	75.754932
172.767361	20.620372	75.759937
172.091109	22.990962	75.764942
171.273020	14.240496	75.769946
170.748373	17.857863	75.774951
169.576615	14.312233	75.779956
169.016656	13.709247	75.784961
168.293620	19.430238	75.789966
167.588735	6.255985	75.794970
166.936124	12.153391	75.799975
166.180541	30.355690	75.804980
165.634546	14.759269	75.809985
165.089505	17.373852	75.814990
164.350835	16.107118	75.819994
163.716952	16.993437	75.824999
162.802813	21.191692	75.830004
162.805080	16.328274	75.835009
161.624368	20.315157	75.840014
160.833488	24.484300	75.845018
160.747648	9.402690	75.850023
159.470464	15.874314	75.855028
158.747935	14.765849	75.860033
158.113411	17.891411	75.865038
157.628934	12.314017	75.870042
157.248560	18.511778	75.875047
156.083185	37.411745	75.880052
155.782925	14.350708	75.885057
155.144173	14.078814	75.890062
154.695340	24.522937	75.895066
153.862258	19.002700	75.900071
153.039363	25.077066	75.905076
152.843799	10.438703	75.910081
151.651335	24.997151	75.915086
150.858622	27.122980	75.920090
150.722954	17.539937	75.925095
149.688648	23.398867	75.930100
148.926117	15.429559	75.935105
148.415035	29.335356	75.940110
147.320421	23.427913	75.945114
147.535439	19.230699	75.950119
146.377554	28.140060	75.955124
145.657257	21.302510	75.960129
145.222508	27.650863	75.965134
145.033375	19.254259	75.970138
143.971761	6.376576	75.975143
143.248612	32.128437	75.980148
142.593820	10.809604	75.985153
141.504256	28.029158	75.990158
140.406757	24.124791	75.995162
140.317896	8.731449	76.000167
139.718305	21.697352	76.005172
139.576103	18.348679	76.010177
139.357236	21.855800	76.015182
138.275337	22.589645	76.020186
137.625647	14.457279	76.025191
136.062040	19.270000	76.030196
135.564352	17.868664	76.035201
135.092986	24.483037	76.040206
134.437509	25.142585	76.045210
134.304120	9.679077	76.050215
132.953499	22.193909	76.055220
132.556195	18.535849	76.060225
131.838000	25.821900	76.065230
131.604720	22.941885	76.070234
130.514620	17.778011	76.075239
129.681828	36.613915	76.080244
129.481301	17.270989	76.085249
129.085809	23.163678	76.090254
128.200789	25.359421	76.095258
127.523577	8.654913	76.100263
126.336212	17.062804	76.105268
126.117211	22.034849	76.110273
125.431276	18.563154	76.115278
124.636665	16.434927	76.120282
124.193405	21.046938	76.125287
123.432472	24.391350	76.130292
122.674076	15.301823	76.135297
121.843210	12.873468	76.140302
121.426239	19.417669	76.145306
120.728595	15.306062	76.150311
119.749057	26.951228	76.155316
119.590091	25.705606	76.160321
118.677892	12.695304	76.165326
117.850119	27.722286	76.170330
117.233816	17.045858	76.175335
116.263723	24.244352	76.180340
116.359625	16.262747	76.185345
115.933601	15.676262	76.190350
114.830475	27.990802	76.195354
114.382396	15.396897	76.200359
113.699185	21.398540	76.205364
112.728995	26.326375	76.210369
112.064388	20.115432	76.215374
111.249666	27.708599	76.220378
111.043585	16.826420	76.225383
109.688915	29.698284	76.230388
109.363017	12.500969	76.235393
108.936452	25.048227	76.240398
108.360799	19.147934	76.245402
107.833285	20.122955	76.250407
106.812907	26.263516	76.255412
106.333789	15.311343	76.260417
105.434675	19.450454	76.265422
104.488630	9.988761	76.270426
104.051185	23.081769	76.275431
103.349935	24.573321	76.280436
103.445406	18.460362	76.285441
102.224523	22.731204	76.290446
101.388584	30.641554	76.295450
100.956757	15.594621	76.300455
100.525236	20.956925	76.305460
99.947600	13.207298	76.310465
99.021551	22.618991	76.315470
97.911368	29.879254	76.320474
97.201564	23.511529	76.325479
96.036020	25.051891	76.330484
95.945782	16.705754	76.335489
95.604997	20.891445	76.340494
94.856827	17.424954	76.345498
95.092553	18.554218	76.350503
93.979162	19.676281	76.355508
93.548563	26.132781	76.360513
92.900624	21.824032	76.365518
91.535299	25.342098	76.370522
90.838494	20.200676	76.375527
90.282659	17.542405	76.380532
89.205132	24.542010	76.385537
88.784665	26.718877	76.390542
87.824954	25.870592	76.395546
87.886394	22.197730	76.400551
87.358039	20.888021	76.405556
86.705700	18.383903	76.410561
85.822094	20.098493	76.415566
85.212211	23.251681	76.420570
84.557909	22.509227	76.425575
83.531284	17.518169	76.430580
83.398923	17.767900	76.435585
82.574115	22.497530	76.440590
81.591733	22.923811	76.445594
81.059163	16.991427	76.450599
80.445646	23.229530	76.455604
80.136009	14.651895	76.460609
79.030770	20.802842	76.465614
78.012078	13.678611	76.470618
78.160651	11.781590	76.475623
77.198424	13.636446	76.480628
76.463961	11.656330	76.485633
75.941101	22.960612	76.490638
74.873651	14.871236	76.495642
74.115973	16.171533	76.500647
73.173431	28.752197	76.505652
73.163679	18.778524	76.510657
72.753669	26.056439	76.515662
72.345597	21.807209	76.520666
71.020403	23.764103	76.525671
70.204429	25.046892	76.530676
70.183559	18.416356	76.535681
69.381533	15.759507	76.540686
68.215038	17.889778	76.545690
67.629849	10.754765	76.550695
66.910835	25.956786	76.555700
66.922632	18.928402	76.560705
66.001307	4.350617	76.565710
65.233403	26.132774	76.570714
64.926112	9.146963	76.575719
63.997914	25.869320	76.580724
63.279998	24.708112	76.585729
62.838841	11.717331	76.590734
61.867656	19.952010	76.595738
61.062610	20.719003	76.600743
60.246907	25.368345	76.605748
59.582115	16.161420	76.610753
59.647458	17.601687	76.615758
59.048875	21.000644	76.620762
58.082009	14.140955	76.625767
57.164365	12.491238	76.630772
56.918282	18.167728	76.635777
55.727204	9.847361	76.640782
55.052561	14.374862	76.645786
54.712408	18.989361	76.650791
54.066870	15.017690	76.655796
53.710014	6.897001	76.660801
52.694823	24.224553	76.665806
52.163203	13.351731	76.670810
51.641900	17.533101	76.675815
50.311810	23.544888	76.680820
49.898455	15.133602	76.685825
49.280982	14.085682	76.690830
48.949596	21.393633	76.695834
48.105172	8.311066	76.700839
47.149569	21.327449	76.705844
46.571058	23.854359	76.710849
46.401787	13.813098	76.715854
45.381801	24.991676	76.720858
44.652183	17.170115	76.725863
43.984437	22.379301	76.730868
43.767850	18.990464	76.735873
42.177869	27.416876	76.740878
41.662178	20.701265	76.745882
41.617399	12.261161	76.750887
41.010480	22.279522	76.755892
40.785683	19.065449	76.760897
39.624254	17.588652	76.765902
38.914936	20.782937	76.770906
38.277443	20.695365	76.775911
37.519750	23.566227	76.780916
36.691095	10.019129	76.785921
36.185877	16.919590	76.790926
35.415590	22.938291	76.795930
34.664798	20.287473	76.800935
33.707842	28.138297	76.805940
33.907608	19.774298	76.810945
33.599430	16.519912	76.815950
32.207926	21.373051	76.820954
31.783200	25.370299	76.825959
30.812553	22.093843	76.830964
29.800306	21.728595	76.835969
29.140071	25.489032	76.840974
28.568356	31.337304	76.845978
28.559270	21.590595	76.850983
28.018605	15.982774	76.855988
27.032809	25.884958	76.860993
26.373900	25.201598	76.865998
25.574053	25.786435	76.871002
25.012010	9.642312	76.876007
23.748015	17.764440	76.881012
23.156218	28.308642	76.886017
22.784850	21.445446	76.891022
22.390089	19.354399	76.896026
22.188886	19.704994	76.901031
21.113183	22.334862	76.906036
20.695324	23.346024	76.911041
19.739307	16.431008	76.916046
18.516629	23.378101	76.921050
18.313894	10.109627	76.926055
17.511579	24.323635	76.931060
17.469112	18.530705	76.936065
16.093694	16.447846	76.941070
15.715051	24.319968	76.946074
14.975450	19.609574	76.951079
14.426984	16.092336	76.956084
13.581925	17.808687	76.961089
12.819534	24.333882	76.966094
12.275048	14.800300	76.971098
12.329662	6.694412	76.976103
11.235826	17.291875	76.981108
10.582495	27.908968	76.986113
9.976225	21.210967	76.991118
8.627664	20.271780	76.996122
8.387391	18.507735	77.001127
7.610918	19.423143	77.006132
7.377376	9.917236	77.011137
6.318634	14.025071	77.016142
5.683656	22.636626	77.021147
4.936629	21.902676	77.026151
4.318408	23.537121	77.031156
4.180553	18.735482	77.036161