Mon Mar 08 19:04:25 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.979959	102.053842	0.000000
-1.786552	83.762911	0.005005
-2.365540	56.586595	0.010010
-4.053985	-0.060736	0.015014
-8.720560	9.040861	0.020019
-13.639266	6.567580	0.025024
-18.310707	-2.203658	0.030029
-23.186901	1.390337	0.035034
-26.663228	5.385495	0.040038
-30.648423	7.665789	0.045043
-34.254910	-3.050816	0.050048
-37.773481	8.967814	0.055053
-41.648805	7.212779	0.060058
-45.241612	1.989340	0.065062
-49.246313	11.382804	0.070067
-52.855286	-2.146481	0.075072
-56.550716	3.861040	0.080077
-60.713385	11.507338	0.085082
-64.160070	2.767890	0.090086
-67.821362	11.499516	0.095091
-71.886453	5.522029	0.100096
-75.437906	0.225813	0.105101
-79.335640	8.373890	0.110106
-82.801630	0.203642	0.115110
-86.662344	12.680593	0.120115
-90.607140	8.036887	0.125120
-94.345786	3.898010	0.130125
-98.524628	8.454742	0.135130
-101.333491	9.588764	0.140134
-105.412145	4.908095	0.145139
-108.935482	9.896400	0.150144
-112.969202	7.378324	0.155149
-117.291947	5.303733	0.160154
-120.604651	6.699496	0.165158
-124.748236	-4.106304	0.170163
-128.130716	4.005370	0.175168
-131.717547	16.646838	0.180173
-135.746589	13.017949	0.185178
-139.145791	5.225033	0.190182
-143.347835	6.672838	0.195187
-147.236772	-1.549671	0.200192
-151.029982	4.695924	0.205197
-154.759486	15.084790	0.210202
-158.168047	0.169184	0.215206
-161.865899	14.383178	0.220211
-165.372294	-3.976414	0.225216
-169.257908	-6.426565	0.230221
-173.583576	1.225421	0.235226
-177.228524	0.892434	0.240230
-181.725692	1.669929	0.245235
-185.088539	-0.559282	0.250240
-188.455451	10.855068	0.255245
-192.441863	17.601460	0.260250
-195.734257	10.739270	0.265254
-199.499807	9.082084	0.270259
-203.296784	2.525916	0.275264
-207.093596	6.916219	0.280269
-210.911752	5.836688	0.285274
-214.755306	5.436109	0.290278
-218.799549	7.934274	0.295283
-222.118813	3.604104	0.300288
-226.177235	13.236636	0.305293
-229.886961	6.734390	0.310298
-233.424326	-1.091522	0.315302
-237.652421	19.971883	0.320307
-240.903797	1.701013	0.325312
-244.453513	-8.997502	0.330317
-248.710530	8.670837	0.335322
-252.468331	-6.061153	0.340326
-256.496417	8.036947	0.345331
-260.091668	8.202321	0.350336
-263.562806	4.153475	0.355341
-267.301056	14.335753	0.360346
-270.798262	2.323259	0.365350
-274.797998	2.494869	0.370355
-278.444713	12.840736	0.375360
-282.387774	7.085399	0.380365
-286.444940	4.216569	0.385370
-289.895706	5.882163	0.390374
-294.005327	9.392186	0.395379
-297.748117	2.081676	0.400384
-301.295539	-3.594857	0.405389
-305.202866	11.020171	0.410394
-308.563392	10.151584	0.415398
-312.354320	13.990790	0.420403
-316.195676	3.823024	0.425408
-319.798510	0.867540	0.430413
-324.027239	13.707913	0.435418
-327.723359	3.103849	0.440422
-331.691409	3.231075	0.445427
-334.887282	1.161491	0.450432
-338.863963	6.135758	0.455437
-342.899196	3.329752	0.460442
-346.445213	-0.137775	0.465446
-350.404336	4.472609	0.470451
-353.937953	5.780960	0.475456
-357.325371	7.207894	0.480461
-361.421761	4.947811	0.485466
-364.907909	2.090455	0.490470
-369.013454	4.280131	0.495475
-372.900195	-5.514457	0.500480
-376.718646	1.303170	0.505485
-380.425061	-2.411492	0.510490
-383.712750	-5.442417	0.515494
-388.014613	16.180154	0.520499
-391.470541	4.107648	0.525504
-395.263785	-10.528551	0.530509
-399.219779	2.632642	0.535514
-402.640716	-6.952430	0.540518
-406.514475	-1.841535	0.545523
-410.230261	-4.728386	0.550528
-414.055785	3.479629	0.555533
-418.004648	1.820521	0.560538
-421.309767	-3.916590	0.565542
-425.906829	7.027464	0.570547
-429.881189	4.196119	0.575552
-432.680584	-9.095967	0.580557
-436.414058	-2.375392	0.585562
-440.392084	3.288333	0.590566
-443.997568	4.742322	0.595571
-447.960036	5.531123	0.600576
-451.818867	-1.341162	0.605581
-456.317956	4.654931	0.610586
-459.596362	-2.150761	0.615590
-463.027405	4.803820	0.620595
-466.648837	-12.625473	0.625600
-470.192508	1.438167	0.630605
-474.471238	10.737288	0.635610
-477.904772	-6.047109	0.640614
-481.834476	-0.739518	0.645619
-485.627686	-8.912080	0.650624
-489.366586	2.257718	0.655629
-493.220822	-2.346152	0.660634
-496.954247	-6.467870	0.665638
-501.129758	4.249736	0.670643
-504.353762	1.096852	0.675648
-508.058853	-6.350206	0.680653
-512.006836	1.169509	0.685658
-515.132471	-0.283462	0.690662
-519.232638	-0.164787	0.695667
-523.028726	3.820635	0.700672
-526.968413	-0.528274	0.705677
-531.029746	-4.903476	0.710682
-534.615420	-3.925569	0.715686
-538.043136	3.484290	0.720691
-542.028034	-1.306773	0.725696
-545.598752	-6.635455	0.730701
-549.617942	1.789762	0.735706
-553.130891	2.111153	0.740710
-557.597154	2.874953	0.745715
-561.292174	-7.709967	0.750720
-564.322350	-1.697580	0.755725
-568.338253	-5.908096	0.760730
-572.022259	-3.388043	0.765734
-575.579043	-10.229517	0.770739
-579.550527	-3.024466	0.775744
-583.476592	-4.593904	0.780749
-587.666956	4.825322	0.785754
-591.189981	2.461438	0.790758
-594.829009	3.791710	0.795763
-598.327606	1.357709	0.800768
-601.951902	-1.002596	0.805773
-606.050671	7.340816	0.810778
-609.925992	0.960253	0.815782
-613.812319	2.885106	0.820787
-617.070384	6.820996	0.825792
-620.666400	-4.607485	0.830797
-624.733279	10.061884	0.835802
-628.284112	0.105272	0.840806
-632.478266	4.070883	0.845811
-636.202755	7.255045	0.850816
-639.683648	-0.740091	0.855821
-643.739662	5.715380	0.860826
-647.297959	-0.670037	0.865830
-651.178655	9.106649	0.870835
-654.919772	-3.192665	0.875840
-658.484039	-1.276618	0.880845
-662.867357	6.380692	0.885850
-666.233816	-4.207665	0.890854
-669.834121	-4.578569	0.895859
-673.586435	-0.297155	0.900864
-677.081764	1.713554	0.905869
-681.139138	3.497123	0.910874
-684.994689	1.154973	0.915878
-689.102543	0.475711	0.920883
-692.651810	-5.455368	0.925888
-696.108595	8.517431	0.930893
-699.973954	-6.341664	0.935898
-703.539367	-1.989149	0.940902
-707.504294	1.343918	0.945907
-711.496801	7.604863	0.950912
-714.702728	-5.084193	0.955917
-718.643523	6.143429	0.960922
-722.422296	-10.743081	0.965926
-726.427142	14.926030	0.970931
-730.325950	2.131681	0.975936
-734.078855	8.806929	0.980941
-737.983108	2.180489	0.985946
-741.288570	8.345886	0.990950
-745.282876	3.088355	0.995955
-748.724855	4.122463	1.000960
-752.946765	2.510704	1.005965
-756.420378	0.558614	1.010970
-760.056702	4.980888	1.015974
-764.094423	-0.682803	1.020979
-767.634396	4.455738	1.025984
-771.319539	-9.361351	1.030989
-775.342830	5.127828	1.035994
-778.803450	-5.819017	1.040998
-782.942002	9.267298	1.046003
-786.256994	1.165457	1.051008
-790.151335	0.264605	1.056013
-794.346366	2.712139	1.061018
-797.916642	5.053524	1.066022
-801.691985	-0.008684	1.071027
-805.357931	2.497802	1.076032
-808.804561	-4.007701	1.081037
-812.924700	5.399099	1.086042
-816.850720	8.633095	1.091046
-820.742384	0.232420	1.096051
-824.466227	3.520840	1.101056
-827.596758	-5.660592	1.106061
-831.230276	6.153555	1.111066
-835.177218	-1.933928	1.116070
-839.176388	8.349225	1.121075
-843.051245	-3.745474	1.126080
-846.597978	4.024426	1.131085
-850.893098	-3.583205	1.136090
-853.984147	-4.549279	1.141094
-857.684648	1.430275	1.146099
-861.718472	-0.514104	1.151104
-865.501466	8.920887	1.156109
-869.548614	3.169009	1.161114
-873.168566	6.011997	1.166118
-877.127282	1.920599	1.171123
-880.837558	6.681280	1.176128
-884.153881	-1.581036	1.181133
-887.983960	11.977063	1.186138
-891.696389	-5.102670	1.191142
-895.612515	-9.476787	1.196147
-899.412858	5.858394	1.201152
-903.042745	-2.964002	1.206157
-906.954686	11.225332	1.211162
-910.463483	0.797288	1.216166
-914.416949	-2.153253	1.221171
-918.280649	1.611799	1.226176
-921.854870	5.516644	1.231181
-926.045645	3.301023	1.236186
-929.601018	-8.833558	1.241190
-933.111092	3.126563	1.246195
-936.871346	-0.364149	1.251200
-940.597842	1.198238	1.256205
-944.870468	5.802941	1.261210
-948.092011	-0.990631	1.266214
-951.871266	10.373941	1.271219
-955.924685	0.085085	1.276224
-959.348282	-3.385306	1.281229
-963.576983	6.270895	1.286234
-966.787683	-1.607669	1.291238
-970.634583	9.595871	1.296243
-974.577261	4.138113	1.301248
-978.626709	-1.310448	1.306253
-982.815878	1.794020	1.311258
-986.046905	8.417739	1.316262
-989.705883	1.216391	1.321267
-992.867596	5.362864	1.326272
-996.714772	1.152920	1.331277
-1000.834597	8.462790	1.336282
-1004.403717	-6.398973	1.341286
-1009.051443	3.756362	1.346291
-1012.582252	-3.057040	1.351296
-1015.668637	-0.174592	1.356301
-1019.526552	1.997095	1.361306
-1022.967959	-1.058800	1.366310
-1027.111888	2.699205	1.371315
-1030.948891	0.499734	1.376320
-1035.196523	-9.830444	1.381325
-1039.050552	0.756215	1.386330
-1042.348000	1.901667	1.391334
-1045.782871	2.067811	1.396339
-1049.968057	-1.099309	1.401344
-1053.578863	-0.559690	1.406349
-1058.138767	11.948525	1.411354
-1060.730085	-4.652669	1.416358
-1065.089066	-0.486495	1.421363
-1068.571247	5.387504	1.426368
-1072.176256	-0.821048	1.431373
-1076.489610	7.823944	1.436378
-1079.854229	0.310758	1.441382
-1083.888379	14.582981	1.446387
-1087.174278	7.328427	1.451392
-1090.960545	7.705371	1.456397
-1095.039627	12.742974	1.461402
-1098.827946	1.992541	1.466406
-1102.650750	12.041341	1.471411
-1106.460716	6.463244	1.476416
-1109.862094	9.653223	1.481421
-1113.782614	13.790353	1.486426
-1117.671909	12.159165	1.491430
-1121.562992	12.206021	1.496435
-1125.165877	5.109455	1.501440
-1128.374119	-1.394268	1.506445
-1132.462412	-0.000768	1.511450
-1135.893443	9.062964	1.516454
-1140.114886	15.564643	1.521459
-1144.385160	13.579736	1.526464
-1147.616131	-1.509334	1.531469
-1151.767861	-0.318525	1.536474
-1155.231500	1.809231	1.541478
-1158.819028	13.051985	1.546483
-1162.564836	2.856215	1.551488
-1166.252296	2.908415	1.556493
-1170.180778	9.648683	1.561498
-1173.549026	-6.752380	1.566502
-1177.658590	13.322180	1.571507
-1181.684359	9.973686	1.576512
-1185.382236	13.299512	1.581517
-1188.976535	10.593154	1.586522
-1192.374113	9.019031	1.591526
-1196.779326	6.355699	1.596531
-1200.464517	6.943713	1.601536
-1204.454985	7.145370	1.606541
-1208.178023	13.160602	1.611546
-1211.395575	3.361330	1.616550
-1215.247374	11.541665	1.621555
-1218.574457	5.121735	1.626560
-1222.598271	9.335489	1.631565
-1226.981968	6.085344	1.636570
-1230.317988	2.747992	1.641574
-1234.436952	4.671662	1.646579
-1237.789291	10.569281	1.651584
-1241.644586	-0.226950	1.656589
-1245.804101	7.815026	1.661594
-1249.116127	8.991484	1.666598
-1253.102306	8.717912	1.671603
-1256.644061	-1.365276	1.676608
-1260.278749	-2.910816	1.681613
-1264.250858	12.490233	1.686618
-1267.828356	7.241036	1.691622
-1271.765539	21.111721	1.696627
-1275.429956	5.759492	1.701632
-1279.064769	-0.833433	1.706637
-1283.267573	9.114039	1.711642
-1286.990843	2.070116	1.716646
-1290.870970	9.367346	1.721651
-1294.560183	0.868880	1.726656
-1297.882927	17.837505	1.731661
-1301.893738	15.978513	1.736666
-1305.457784	6.577004	1.741670
-1309.434573	14.265021	1.746675
-1313.263425	4.448626	1.751680
-1317.162897	16.807468	1.756685
-1321.153780	17.279031	1.761690
-1324.011902	5.288949	1.766694
-1327.812118	15.914754	1.771699
-1331.728692	5.100105	1.776704
-1335.280232	13.271994	1.781709
-1339.868491	12.784299	1.786714
-1342.978932	9.811522	1.791718
-1346.791375	22.851869	1.796723
-1350.677682	9.585164	1.801728
-1354.516101	0.429490	1.806733
-1358.532385	16.943116	1.811738
-1361.808421	13.091769	1.816742
-1365.978477	14.107710	1.821747
-1369.751268	8.204015	1.826752
-1373.020936	10.936507	1.831757
-1377.345694	2.957769	1.836762
-1380.468185	7.543138	1.841766
-1384.290363	5.535835	1.846771
-1388.463863	10.499171	1.851776
-1391.608471	10.185735	1.856781
-1396.245568	15.280062	1.861786
-1399.652151	5.662707	1.866790
-1403.755510	8.290596	1.871795
-1407.038454	9.454738	1.876800
-1410.683057	9.030572	1.881805
-1414.917272	15.126377	1.886810
-1418.535833	4.719882	1.891814
-1422.166242	10.001580	1.896819
-1426.181095	7.064904	1.901824
-1429.691855	8.536764	1.906829
-1433.466411	11.917826	1.911834
-1436.945406	-0.453630	1.916838
-1440.594599	8.637564	1.921843
-1444.719893	7.755864	1.926848
-1448.387186	-2.686924	1.931853
-1452.530728	11.135074	1.936858
-1456.122662	2.099376	1.941862
-1460.218412	8.192012	1.946867
-1463.713116	15.924514	1.951872
-1467.225628	8.339411	1.956877
-1471.276639	13.912436	1.961882
-1474.901155	10.205353	1.966886
-1478.525166	10.747746	1.971891
-1482.438832	10.103444	1.976896
-1486.109364	6.282332	1.981901
-1490.499260	20.590089	1.986906
-1493.218268	6.321523	1.991910
-1497.065358	9.799450	1.996915
-1501.193470	5.499951	2.006912
-1502.335905	4.959747	2.016909
-1499.928740	10.741255	2.026906
-1497.187076	10.002253	2.036902
-1494.942048	13.911956	2.046899
-1493.012847	11.953136	2.056896
-1490.971935	14.411411	2.066893
-1489.146690	14.636996	2.076890
-1487.401031	12.852823	2.086886
-1485.345381	11.336365	2.096883
-1483.571090	11.180138	2.106880
-1481.312714	6.173550	2.116877
-1479.780059	15.213326	2.126874
-1478.018138	14.492277	2.136870
-1475.797953	4.360558	2.146867
-1473.933462	12.256223	2.156864
-1472.344117	10.834962	2.166861
-1470.201196	8.628798	2.176858
-1468.365629	5.829256	2.186854
-1466.286798	2.465011	2.196851
-1464.447579	7.579644	2.206848
-1462.676692	4.539425	2.216845
-1460.683845	4.078241	2.226842
-1459.182596	12.515203	2.236838
-1457.033406	7.232453	2.246835
-1455.127835	7.975697	2.256832
-1453.301891	9.167453	2.266829
-1451.273703	8.833241	2.276826
-1449.354987	3.154795	2.286822
-1447.634119	3.352915	2.296819
-1445.877413	6.376172	2.306816
-1443.681130	2.974197	2.316813
-1441.925017	-0.306783	2.326810
-1439.996694	0.331785	2.336806
-1438.221829	-2.128036	2.346803
-1436.325417	3.217447	2.356800
-1434.418976	4.344229	2.366797
-1432.281116	5.953404	2.376794
-1430.523949	4.967906	2.386790
-1428.787790	5.479363	2.396787
-1426.947938	6.847323	2.406784
-1425.153802	3.416592	2.416781
-1423.163081	2.242142	2.426778
-1421.035714	5.468168	2.436774
-1419.219897	8.196211	2.446771
-1417.544410	8.543716	2.456768
-1415.722452	6.905267	2.466765
-1413.945013	12.012467	2.476762
-1411.844308	13.354470	2.486758
-1409.845176	5.839610	2.496755
-1408.007713	7.612153	2.506752
-1406.263102	9.165892	2.516749
-1404.334601	3.095938	2.526746
-1402.276334	0.941280	2.536742
-1400.458856	1.573943	2.546739
-1398.585544	-4.581900	2.556736
-1396.765960	3.878351	2.566733
-1395.015680	4.376521	2.576730
-1393.146674	6.085609	2.586726
-1391.343564	-1.686784	2.596723
-1389.255410	3.460691	2.606720
-1387.225784	6.198743	2.616717
-1385.611943	7.037687	2.626714
-1383.870627	-2.946247	2.636710
-1381.729761	7.597192	2.646707
-1379.840105	6.276334	2.656704
-1377.812137	5.686449	2.666701
-1376.262018	4.819392	2.676698
-1374.125151	2.178523	2.686694
-1372.381433	4.600797	2.696691
-1370.408019	6.638959	2.706688
-1368.865747	4.434300	2.716685
-1366.915589	6.547237	2.726682
-1364.962783	10.770671	2.736678
-1362.960750	3.661149	2.746675
-1360.986607	4.824521	2.756672
-1359.144527	5.571692	2.766669
-1357.556201	3.086528	2.776666
-1355.550281	14.579962	2.786662
-1353.602805	4.059392	2.796659
-1351.369908	3.599351	2.806656
-1350.055606	0.720711	2.816653
-1348.092481	1.873227	2.826650
-1345.889335	10.172667	2.836646
-1344.251196	5.412312	2.846643
-1342.392852	2.565013	2.856640
-1340.443091	5.915853	2.866637
-1338.532705	8.186749	2.876634
-1336.780787	3.813953	2.886630
-1335.155862	4.670105	2.896627
-1332.753522	5.727076	2.906624
-1330.951382	4.410791	2.916621
-1329.124257	2.968938	2.926618
-1327.379678	1.407675	2.936614
-1325.393243	1.833366	2.946611
-1323.456227	5.449928	2.956608
-1321.944988	8.600985	2.966605
-1320.065721	7.390779	2.976602
-1317.870483	5.332686	2.986598
-1315.725746	4.462078	2.996595
-1314.341085	4.990404	3.006592
-1312.335734	3.826337	3.016589
-1310.223301	4.625011	3.026586
-1308.785561	3.864399	3.036582
-1306.715225	2.873083	3.046579
-1304.507429	8.899859	3.056576
-1302.723617	9.226954	3.066573
-1301.321534	9.117803	3.076570
-1299.262148	10.313373	3.086566
-1296.966220	2.190614	3.096563
-1295.376666	8.788414	3.106560
-1293.743122	7.142319	3.116557
-1291.680724	10.047309	3.126554
-1289.943000	5.083170	3.136550
-1287.979215	6.688762	3.146547
-1285.766995	6.522600	3.156544
-1284.070688	-0.024807	3.166541
-1282.268235	10.209759	3.176538
-1280.490037	7.367438	3.186534
-1278.453768	6.411597	3.196531
-1276.599954	8.282677	3.206528
-1274.764670	7.862654	3.216525
-1273.112705	15.209915	3.226522
-1271.119918	8.553493	3.236518
-1269.037644	5.029403	3.246515
-1267.221872	10.015334	3.256512
-1265.395831	5.564415	3.266509
-1263.475327	1.570459	3.276506
-1261.600705	11.180901	3.286502
-1259.757487	14.893053	3.296499
-1257.705048	11.852137	3.306496
-1256.010116	11.621947	3.316493
-1254.071785	5.168452	3.326490
-1252.099949	5.173412	3.336486
-1250.389790	11.185142	3.346483
-1248.464790	9.247719	3.356480
-1246.699965	11.589351	3.366477
-1244.651986	8.336016	3.376474
-1243.088848	13.400285	3.386470
-1240.933302	6.640481	3.396467
-1239.102328	6.254333	3.406464
-1237.068080	5.744086	3.416461
-1235.219695	5.831967	3.426458
-1233.616467	5.089130	3.436454
-1231.491724	8.746784	3.446451
-1229.918004	5.332519	3.456448
-1227.659984	5.490644	3.466445
-1226.233034	7.933718	3.476442
-1223.869349	12.369415	3.486438
-1222.181881	11.982558	3.496435
-1220.328139	10.375487	3.506432
-1218.285383	7.178270	3.516429
-1216.895620	1.635158	3.526426
-1214.794418	7.323838	3.536422
-1212.863144	10.106205	3.546419
-1210.649158	10.520850	3.556416
-1209.117254	10.015217	3.566413
-1207.371187	11.205741	3.576410
-1205.579037	11.979971	3.586406
-1203.299008	7.456461	3.596403
-1201.495184	4.019609	3.606400
-1199.568558	5.640695	3.616397
-1197.829742	0.981165	3.626394
-1196.194015	2.849309	3.636390
-1193.974947	3.319995	3.646387
-1192.079832	1.741062	3.656384
-1190.327270	4.408364	3.666381
-1188.581826	9.378772	3.676378
-1186.578046	2.734870	3.686374
-1184.623598	5.156732	3.696371
-1182.704750	-0.516794	3.706368
-1180.745756	2.412734	3.716365
-1179.149851	6.530810	3.726362
-1177.346299	2.820878	3.736358
-1175.173875	8.741346	3.746355
-1173.376431	7.070691	3.756352
-1171.711435	10.123047	3.766349
-1169.992100	17.312780	3.776346
-1167.844360	8.479673	3.786342
-1165.858776	11.652842	3.796339
-1163.909118	9.653125	3.806336
-1162.001416	6.744387	3.816333
-1160.388000	4.176396	3.826330
-1158.550803	9.560019	3.836326
-1156.361245	9.498652	3.846323
-1154.495607	8.406014	3.856320
-1152.672888	4.202011	3.866317
-1151.041988	4.547369	3.876314
-1148.961829	13.376660	3.886310
-1147.340481	6.353466	3.896307
-1145.380347	4.749959	3.906304
-1143.356431	-0.905610	3.916301
-1141.487849	-0.074088	3.926298
-1139.592759	11.778320	3.936294
-1137.712896	11.431795	3.946291
-1136.131096	3.666559	3.956288
-1133.863001	2.111688	3.966285
-1132.104751	7.151140	3.976282
-1130.075139	10.241512	3.986278
-1128.374220	3.589264	3.996275
-1126.616236	9.149785	4.006272
-1124.625194	11.142714	4.016269
-1122.717139	4.960989	4.026266
-1121.112974	9.876687	4.036262
-1118.935222	14.089621	4.046259
-1117.123163	10.995702	4.056256
-1115.125936	3.847671	4.066253
-1113.280477	9.910496	4.076250
-1111.335302	11.081876	4.086246
-1109.639131	12.010472	4.096243
-1108.015819	11.313452	4.106240
-1105.958392	15.487228	4.116237
-1103.751766	15.331608	4.126234
-1102.136507	19.644006	4.136230
-1100.158691	16.692523	4.146227
-1098.539959	9.723456	4.156224
-1096.399818	6.965475	4.166221
-1094.463473	10.954955	4.176218
-1092.832010	6.734221	4.186214
-1091.252589	7.091012	4.196211
-1088.770157	10.928420	4.206208
-1086.862455	17.077626	4.216205
-1085.294418	3.123934	4.226202
-1083.272894	3.792102	4.236198
-1081.407664	11.072247	4.246195
-1079.687626	13.005935	4.256192
-1077.629882	5.227764	4.266189
-1075.999022	-2.617908	4.276186
-1073.703777	6.303361	4.286182
-1072.142446	10.071805	4.296179
-1070.289218	5.330908	4.306176
-1068.468753	-2.115636	4.316173
-1066.358293	4.329555	4.326170
-1064.793975	8.585391	4.336166
-1062.725192	10.040183	4.346163
-1060.770897	3.465869	4.356160
-1058.938539	0.141394	4.366157
-1057.198333	2.450797	4.376154
-1054.994077	10.852989	4.386150
-1053.322034	14.167977	4.396147
-1051.554020	-3.605345	4.406144
-1049.527292	2.194871	4.416141
-1047.415231	12.793792	4.426138
-1045.678698	6.289050	4.436134
-1044.197895	13.179156	4.446131
-1042.081236	13.293756	4.456128
-1039.988447	8.195641	4.466125
-1038.350228	11.880764	4.476122
-1036.690022	7.876508	4.486118
-1034.323150	10.526212	4.496115
-1032.701916	10.810045	4.506112
-1030.627612	10.801963	4.516109
-1029.103821	14.986944	4.526106
-1027.125953	11.276084	4.536102
-1025.187895	11.866077	4.546099
-1023.390616	13.732196	4.556096
-1021.290867	11.970682	4.566093
-1019.880956	3.610934	4.576090
-1017.960168	11.036977	4.586086
-1015.711808	7.300239	4.596083
-1013.823608	9.349182	4.606080
-1012.038592	6.883314	4.616077
-1010.054708	6.656039	4.626074
-1008.210019	7.718845	4.636070
-1006.464106	8.549567	4.646067
-1004.377658	1.774175	4.656064
-1002.613650	8.181679	4.666061
-1000.895574	3.767165	4.676058
-998.867757	1.852973	4.686054
-997.030003	8.796552	4.696051
-995.188889	-0.281044	4.706048
-993.519268	-0.612780	4.716045
-991.184671	2.195277	4.726042
-989.530962	4.108061	4.736038
-987.668968	3.794513	4.746035
-985.977263	-1.806229	4.756032
-983.926675	4.815975	4.766029
-981.709691	3.217319	4.776026
-980.282230	4.297917	4.786022
-978.362341	10.355272	4.796019
-976.389224	7.744097	4.806016
-974.423783	8.276073	4.816013
-972.564502	5.097348	4.826010
-970.596413	2.927482	4.836006
-968.901830	7.948828	4.846003
-967.229800	11.814902	4.856000
-965.300790	10.451769	4.865997
-963.229812	9.864838	4.875994
-961.294121	0.912662	4.885990
-959.244122	12.701001	4.895987
-957.496356	4.445149	4.905984
-955.872893	5.301804	4.915981
-954.070150	7.718123	4.925978
-952.170201	8.014288	4.935974
-949.916365	6.308722	4.945971
-948.174058	5.302277	4.955968
-946.434625	1.369095	4.965965
-944.510350	5.228011	4.975962
-942.838370	7.224746	4.985958
-940.916813	5.529685	4.995955
-938.593658	1.552126	5.005952
-937.070256	0.713312	5.015949
-935.110783	7.564856	5.025946
-933.251039	10.668355	5.035942
-931.431052	5.748149	5.045939
-929.263809	1.640798	5.055936
-927.572305	3.639158	5.065933
-925.780755	1.677544	5.075930
-923.890772	4.305715	5.085926
-921.930287	9.938234	5.095923
-920.046770	10.252840	5.105920
-918.227470	4.224397	5.115917
-916.421114	11.747769	5.125914
-914.668593	14.268461	5.135910
-912.714939	10.951542	5.145907
-910.661863	10.748024	5.155904
-908.704789	4.784398	5.165901
-906.807407	5.131533	5.175898
-905.171907	8.267747	5.185894
-903.335019	10.075525	5.195891
-901.529808	11.121045	5.205888
-899.121563	0.107166	5.215885
-897.518935	1.958714	5.225882
-895.745566	6.234931	5.235878
-893.707120	4.218082	5.245875
-891.939418	7.401062	5.255872
-890.189625	8.474396	5.265869
-888.426198	8.448246	5.275866
-886.235042	10.720427	5.285862
-884.400872	-0.013782	5.295859
-882.620241	4.521796	5.305856
-880.530904	9.914292	5.315853
-878.709566	12.646629	5.325850
-877.187344	6.157311	5.335846
-875.065978	9.526914	5.345843
-873.148578	10.822927	5.355840
-871.159942	3.073335	5.365837
-869.532739	-0.039794	5.375834
-867.476350	10.452952	5.385830
-865.658080	13.239472	5.395827
-864.070735	3.506252	5.405824
-861.954789	-1.660146	5.415821
-860.131891	3.999155	5.425818
-858.131270	2.809387	5.435814
-856.169758	1.123797	5.445811
-854.466667	4.148195	5.455808
-852.591801	-1.642780	5.465805
-850.522574	9.348428	5.475802
-848.765818	6.849304	5.485798
-846.996293	3.348724	5.495795
-845.108886	5.577923	5.505792
-843.045005	4.106493	5.515789
-841.188252	6.489007	5.525786
-839.690189	12.879160	5.535782
-837.645779	12.970758	5.545779
-835.731811	6.905136	5.555776
-833.430638	6.226266	5.565773
-832.064115	4.547380	5.575770
-830.169730	6.308133	5.585766
-828.247283	10.762673	5.595763
-826.296604	6.664763	5.605760
-824.385465	8.809665	5.615757
-822.543569	7.263212	5.625754
-820.470732	1.328519	5.635750
-818.998742	8.534384	5.645747
-816.775399	5.382846	5.655744
-814.859744	4.566675	5.665741
-813.200244	6.118682	5.675738
-811.575707	10.622429	5.685734
-809.528015	14.979604	5.695731
-807.333662	10.831710	5.705728
-805.616970	8.904252	5.715725
-803.826391	7.386541	5.725722
-801.679767	3.669417	5.735718
-800.046993	13.012636	5.745715
-798.454442	12.514944	5.755712
-796.319896	6.478832	5.765709
-793.813228	9.343272	5.775706
-792.487585	12.865387	5.785702
-790.844389	16.368330	5.795699
-788.579382	10.676089	5.805696
-786.834541	9.222539	5.815693
-784.991828	10.934750	5.825690
-783.063007	12.884240	5.835686
-781.446165	16.205096	5.845683
-779.582892	14.972611	5.855680
-777.526727	7.280186	5.865677
-775.457144	3.733282	5.875674
-773.642089	4.861007	5.885670
-771.955340	13.579868	5.895667
-769.875620	9.467696	5.905664
-768.170129	5.742155	5.915661
-766.075482	8.418273	5.925658
-764.343467	9.772422	5.935654
-762.557840	14.204676	5.945651
-760.809956	7.466216	5.955648
-758.694127	7.546470	5.965645
-756.966443	4.624188	5.975642
-754.813863	5.304853	5.985638
-753.347575	5.215768	5.995635
-751.231585	7.686396	6.005632
-749.337177	8.814090	6.015629
-747.384969	5.470693	6.025626
-745.576917	6.826915	6.035622
-743.680219	11.944027	6.045619
-741.689593	7.936110	6.055616
-740.107578	12.303029	6.065613
-737.852672	8.634968	6.075610
-736.007052	10.692524	6.085606
-734.706067	3.633938	6.095603
-732.832508	6.185951	6.105600
-730.615594	7.748415	6.115597
-728.445557	0.985151	6.125594
-726.710059	5.174402	6.135590
-725.134088	6.766661	6.145587
-723.116463	13.607529	6.155584
-721.106433	17.342418	6.165581
-719.314906	8.877631	6.175578
-717.388576	7.570386	6.185574
-715.489619	9.906788	6.195571
-713.664896	6.245912	6.205568
-711.559406	8.527211	6.215565
-710.071897	8.815268	6.225562
-708.232364	4.826784	6.235558
-706.277541	5.813815	6.245555
-704.421452	8.594419	6.255552
-702.514748	1.931671	6.265549
-700.418762	7.897979	6.275546
-698.482015	2.240904	6.285542
-696.878607	6.787582	6.295539
-695.100127	5.166101	6.305536
-693.279304	9.082814	6.315533
-691.014835	9.298844	6.325530
-689.039563	10.257360	6.335526
-687.583377	7.078521	6.345523
-685.749698	7.567058	6.355520
-683.326128	15.012541	6.365517
-681.848922	4.526536	6.375514
-679.941934	4.059207	6.385510
-678.068478	4.332986	6.395507
-676.074588	5.498526	6.405504
-674.383755	7.566652	6.415501
-672.279576	7.937775	6.425498
-670.693600	2.733057	6.435494
-668.818304	7.760498	6.445491
-666.864429	13.552188	6.455488
-664.817675	8.226489	6.465485
-663.006867	2.308524	6.475482
-661.002500	3.849751	6.485478
-659.059646	8.189076	6.495475
-657.360757	9.395448	6.505472
-655.641411	5.312526	6.515469
-654.029151	9.494684	6.525466
-652.086592	7.108114	6.535462
-649.738666	6.677727	6.545459
-647.942600	8.754322	6.555456
-645.849113	8.876138	6.565453
-644.423358	6.101638	6.575450
-642.435284	5.880318	6.585446
-640.637547	14.137894	6.595443
-638.580996	9.279573	6.605440
-636.728910	7.404810	6.615437
-634.918331	4.887768	6.625434
-632.749039	4.181215	6.635430
-631.068803	8.510416	6.645427
-629.436141	9.152682	6.655424
-627.892060	11.994246	6.665421
-625.687070	11.179370	6.675418
-623.325978	8.659650	6.685414
-621.743131	7.899956	6.695411
-619.479194	10.860202	6.705408
-618.022171	10.068508	6.715405
-616.299327	2.713653	6.725402
-614.410588	5.713313	6.735398
-612.503676	9.343196	6.745395
-610.388529	5.659684	6.755392
-608.631941	12.144484	6.765389
-606.782256	6.010357	6.775386
-604.809217	8.674472	6.785382
-603.176184	0.705586	6.795379
-601.434127	6.125399	6.805376
-599.246123	9.729338	6.815373
-597.180178	6.328420	6.825370
-595.291890	7.995609	6.835366
-593.582111	6.228869	6.845363
-591.884573	8.367033	6.855360
-589.793285	13.222680	6.865357
-587.881354	8.586438	6.875354
-586.311624	7.577823	6.885350
-584.349183	8.437430	6.895347
-582.163983	3.282306	6.905344
-580.218453	10.291128	6.915341
-578.455029	4.606567	6.925338
-576.680803	5.832541	6.935334
-575.435114	14.083620	6.945331
-573.108640	14.057766	6.955328
-570.998622	8.128384	6.965325
-569.265065	9.970301	6.975322
-567.233372	4.159219	6.985318
-565.356587	11.696902	6.995315
-563.580716	9.483860	7.005312
-561.639423	9.887415	7.015309
-559.882372	9.355713	7.025306
-558.084457	10.557393	7.035302
-556.161057	7.616620	7.045299
-554.102466	6.630993	7.055296
-552.315433	9.763786	7.065293
-550.481966	7.419982	7.075290
-548.958472	4.985169	7.085286
-546.804393	7.530423	7.095283
-544.660702	9.966818	7.105280
-542.806963	6.438793	7.115277
-541.229906	7.405774	7.125274
-539.251392	11.883185	7.135270
-537.110247	7.357207	7.145267
-535.305268	4.462205	7.155264
-533.829409	12.075001	7.165261
-531.615947	8.236913	7.175258
-529.611689	6.971053	7.185254
-527.992035	6.050814	7.195251
-526.322614	15.408924	7.205248
-524.214161	9.353521	7.215245
-522.415381	10.007224	7.225242
-520.491947	6.607025	7.235238
-518.429858	12.207889	7.245235
-516.820116	11.835527	7.255232
-514.767273	9.508817	7.265229
-512.876786	2.356190	7.275226
-511.160453	5.797132	7.285222
-509.170115	4.080377	7.295219
-507.460469	6.715590	7.305216
-505.169675	1.441043	7.315213
-503.250719	-4.573022	7.325210
-501.683384	-2.818189	7.335206
-499.955535	2.982899	7.345203
-497.760548	7.222102	7.355200
-496.333371	2.360201	7.365197
-494.464185	7.088781	7.375194
-491.807700	7.435019	7.385190
-490.457164	2.519048	7.395187
-488.647549	4.615707	7.405184
-486.865215	2.796405	7.415181
-484.610538	1.395860	7.425178
-482.714335	-0.277420	7.435174
-481.029274	11.991230	7.445171
-479.192598	2.666809	7.455168
-477.215735	3.761031	7.465165
-475.603102	-0.203680	7.475162
-473.416979	4.635350	7.485158
-471.730803	-1.736238	7.495155
-470.057527	7.798130	7.505152
-467.668148	7.190785	7.515149
-466.264730	7.006132	7.525146
-463.823222	3.425360	7.535142
-462.338039	7.962667	7.545139
-460.616301	6.694610	7.555136
-458.291100	9.324721	7.565133
-456.687727	8.733954	7.575130
-454.686121	4.699251	7.585126
-452.929095	3.989220	7.595123
-450.894848	4.458544	7.605120
-449.053894	7.671223	7.615117
-447.131021	4.345377	7.625114
-445.668777	2.304072	7.635110
-443.507635	2.917343	7.645107
-441.619239	10.323812	7.655104
-439.799693	11.891583	7.665101
-437.909551	9.388821	7.675098
-435.966253	2.308339	7.685094
-434.231958	5.817520	7.695091
-432.008333	8.789122	7.705088
-430.256225	7.430979	7.715085
-428.550978	3.637816	7.725082
-426.630977	6.354759	7.735078
-424.654751	5.972889	7.745075
-423.046273	9.307967	7.755072
-420.889308	7.031023	7.765069
-418.922110	3.317615	7.775066
-417.398379	9.025052	7.785062
-415.699971	8.504397	7.795059
-413.539377	5.816376	7.805056
-411.624804	10.975125	7.815053
-409.636674	8.829352	7.825050
-407.781792	6.537496	7.835046
-405.867111	1.864638	7.845043
-404.185982	3.261914	7.855040
-402.105721	7.451635	7.865037
-400.546915	10.535725	7.875034
-398.401784	10.840557	7.885030
-396.467019	6.571846	7.895027
-394.585147	7.769720	7.905024
-392.928718	12.518144	7.915021
-391.115495	7.566246	7.925018
-389.287749	10.046911	7.935014
-387.346058	8.966410	7.945011
-385.082706	10.554944	7.955008
-383.426871	6.589708	7.965005
-381.494723	6.626994	7.975002
-379.640717	5.053683	7.984998
-377.729693	11.458753	7.994995
-376.054052	11.930131	8.004992
-374.193062	9.694164	8.014989
-372.097940	11.707442	8.024986
-370.233050	-1.249644	8.034982
-368.627725	-0.677040	8.044979
-366.448835	3.192245	8.054976
-364.663897	2.458876	8.064973
-362.672176	4.551823	8.074970
-361.137190	7.699740	8.084966
-358.955896	5.670006	8.094963
-356.967916	8.665089	8.104960
-355.531292	10.243530	8.114957
-353.690871	10.216538	8.124954
-351.345745	6.433378	8.134950
-349.643281	3.545402	8.144947
-347.768985	13.587755	8.154944
-345.938777	12.049844	8.164941
-343.990180	11.302996	8.174938
-342.271841	10.242396	8.184934
-340.228707	12.164534	8.194931
-338.454082	14.127956	8.204928
-336.598502	7.435738	8.214925
-334.732308	14.113253	8.224922
-332.811868	9.717409	8.234918
-331.004796	11.694604	8.244915
-329.084588	10.184969	8.254912
-327.246702	8.446910	8.264909
-325.360268	7.948408	8.274906
-323.572871	5.578970	8.284902
-321.452252	6.980359	8.294899
-319.468794	4.225963	8.304896
-317.933980	4.741965	8.314893
-315.915275	-2.309413	8.324890
-313.831085	3.000755	8.334886
-311.958688	6.909542	8.344883
-310.413327	7.513861	8.354880
-308.703838	8.286184	8.364877
-306.564318	10.838723	8.374874
-304.671547	-1.252816	8.384870
-302.811314	-0.774537	8.394867
-300.949568	10.935563	8.404864
-298.893213	10.983089	8.414861
-297.067086	8.100672	8.424858
-295.351678	8.753644	8.434854
-293.442537	2.755506	8.444851
-291.402314	4.135019	8.454848
-289.762132	-0.029752	8.464845
-287.677382	7.527080	8.474842
-285.796804	0.845121	8.484838
-284.204429	5.474380	8.494835
-282.107635	2.275629	8.504832
-280.271866	12.117359	8.514829
-278.598003	11.079692	8.524826
-276.530779	3.782188	8.534822
-274.525794	8.691372	8.544819
-272.577373	6.173119	8.554816
-270.957436	2.393677	8.564813
-269.094568	4.521479	8.574810
-266.952206	-6.042051	8.584807
-265.306519	6.446207	8.594803
-263.489031	0.210101	8.604800
-261.649584	4.882044	8.614797
-259.702857	-0.907341	8.624794
-257.446526	0.012995	8.634791
-255.428047	-6.487274	8.644787
-253.837521	-8.296320	8.654784
-252.207540	-3.638308	8.664781
-250.286935	-2.741750	8.674778
-248.424831	-2.682127	8.684775
-246.597202	-1.851250	8.694771
-244.713370	-1.520368	8.704768
-242.719928	6.914718	8.714765
-240.787186	0.672864	8.724762
-238.840105	-2.722997	8.734759
-237.110466	-7.740387	8.744755
-235.102774	-6.000390	8.754752
-233.322139	2.546028	8.764749
-231.591194	-4.339369	8.774746
-229.603976	-5.788569	8.784743
-227.690821	-10.265267	8.794739
-226.073569	-2.990601	8.804736
-224.059876	-6.403397	8.814733
-222.051601	-10.145308	8.824730
-220.140690	-3.692724	8.834727
-218.424726	-2.330874	8.844723
-216.400192	6.222427	8.854720
-214.476388	4.306539	8.864717
-212.933413	-0.741047	8.874714
-210.868698	1.035659	8.884711
-208.977693	-3.806948	8.894707
-207.091533	1.189147	8.904704
-205.300347	0.469107	8.914701
-203.027693	-2.272926	8.924698
-201.362110	2.166296	8.934695
-199.779295	-1.670331	8.944691
-197.829904	-8.857391	8.954688
-195.873216	2.387670	8.964685
-193.766807	-4.617612	8.974682
-192.381264	-8.759054	8.984679
-190.156212	-6.508993	8.994675
-188.250805	-4.495279	9.004672
-186.574390	-3.910214	9.014669
-184.650169	-5.785093	9.024666
-182.702012	-5.849671	9.034663
-180.577161	-9.799616	9.044659
-179.038002	-1.091472	9.054656
-177.049722	-6.607964	9.064653
-175.090003	0.523680	9.074650
-173.442501	-12.494896	9.084647
-171.679215	-8.271761	9.094643
-169.548414	-5.011955	9.104640
-167.687995	-7.996058	9.114637
-165.758786	-7.187643	9.124634
-163.851013	-6.986828	9.134631
-162.155808	-1.260790	9.144627
-160.445093	-0.595920	9.154624
-158.627981	3.332866	9.164621
-156.204825	4.502982	9.174618
-154.466388	-3.580344	9.184615
-152.753404	-0.062814	9.194611
-150.872699	-6.421027	9.204608
-148.729108	-1.156500	9.214605
-146.935979	-1.141054	9.224602
-145.365176	-2.951621	9.234599
-143.690351	-1.570521	9.244595
-141.230582	-0.221504	9.254592
-139.529519	3.214258	9.264589
-137.714778	0.133258	9.274586
-135.947437	0.178089	9.284583
-133.927311	-2.266237	9.294579
-131.997154	-3.357324	9.304576
-129.920506	-2.975015	9.314573
-128.343694	-0.076762	9.324570
-126.570697	-5.952008	9.334567
-124.493173	-0.627972	9.344563
-122.489710	6.487270	9.354560
-120.784767	-7.855646	9.364557
-118.987306	0.912382	9.374554
-117.255102	-1.883870	9.384551
-115.084588	0.258127	9.394547
-113.364780	1.591021	9.404544
-111.520860	0.275298	9.414541
-109.398023	-2.539061	9.424538
-107.521950	-2.153152	9.434535
-105.646444	-2.097136	9.444531
-103.951354	-3.633835	9.454528
-102.364116	-0.094628	9.464525
-100.309392	1.079061	9.474522
-98.223772	-0.314683	9.484519
-96.364225	-0.428210	9.494515
-94.224174	0.518725	9.504512
-93.115126	5.623099	9.514509
-90.798637	3.290996	9.524506
-88.871115	-2.657822	9.534503
-86.760255	-0.269452	9.544499
-85.206115	-3.970388	9.554496
-83.266518	0.150485	9.564493
-81.397122	1.401121	9.574490
-79.461984	2.541803	9.584487
-77.875223	3.575436	9.594483
-75.717222	-3.794808	9.604480
-73.959825	7.685836	9.614477
-71.950674	3.684965	9.624474
-70.072241	3.768962	9.634471
-68.327433	3.740072	9.644467
-66.292808	-0.657996	9.654464
-64.537765	3.530226	9.664461
-62.600380	1.647025	9.674458
-60.695133	0.607333	9.684455
-59.024648	-2.059040	9.694451
-56.947686	-0.382044	9.704448
-55.037310	-2.927214	9.714445
-53.389240	-4.680578	9.724442
-51.295408	1.046694	9.734439
-49.483672	5.615867	9.744435
-47.836097	3.489972	9.754432
-45.581494	5.260217	9.764429
-43.877458	2.408510	9.774426
-41.937118	5.111475	9.784423
-40.152316	4.013645	9.794419
-38.110991	-2.497999	9.804416
-36.106558	3.944566	9.814413
-34.765211	6.672031	9.824410
-32.898209	-0.904384	9.834407
-30.642432	6.849611	9.844403
-28.752029	5.670212	9.854400
-26.867482	2.350798	9.864397
-25.400500	-2.101953	9.874394
-23.205872	1.454108	9.884391
-21.189120	11.691913	9.894387
-19.404834	13.035117	9.904384
-17.792727	5.030440	9.914381
-15.930593	5.199180	9.924378
-13.928890	7.696601	9.934375
-11.751487	8.160833	9.944371
-10.211198	3.461144	9.954368
-8.102652	5.148935	9.964365
-6.349347	5.791334	9.974362
-4.653745	15.267258	9.984359
-3.519313	35.903765	9.994355
-2.403084	92.735871	10.004352
-1.210540	155.585804	10.014349
0.000000	219.342408	10.019354
0.591430	256.924434	10.024359
1.559448	293.284331	10.029363
1.749603	331.466691	10.034368
2.073940	354.085901	10.039373
2.488871	375.649949	10.044378
2.785129	394.187969	10.049383
3.048200	409.017712	10.054387
2.935920	429.328715	10.059392
3.453894	434.659590	10.064397
3.536808	447.587980	10.069402
3.420965	447.527600	10.074407
3.781252	465.995578	10.079411
3.830417	477.294129	10.084416
4.489723	486.915318	10.089421
4.503909	483.722964	10.094426
4.312698	486.188191	10.099431
4.430743	493.746388	10.104435
4.012391	498.004517	10.109440
4.482350	490.194826	10.114445
4.861524	511.955585	10.119450
4.642786	486.184375	10.124455
4.264812	483.254833	10.129459
4.211933	487.189750	10.134464
4.457077	505.871680	10.139469
4.478397	518.865150	10.144474
4.704436	511.275694	10.149479
4.798268	513.797964	10.154483
4.578918	524.540151	10.159488
5.204378	520.411382	10.164493
5.175131	527.807012	10.169498
4.752819	514.746583	10.174503
5.105725	528.451977	10.179507
4.870269	529.235397	10.184512
5.067955	533.928282	10.189517
5.102196	528.572352	10.194522
5.013981	529.598787	10.199527
5.307733	523.718935	10.204531
5.251883	539.515861	10.209536
5.333474	538.498345	10.214541
5.380792	541.553149	10.219546
5.333560	538.156119	10.224551
5.472589	542.145597	10.229555
5.473249	538.584814	10.234560
5.575692	546.468794	10.239565
5.359885	534.660594	10.244570
5.313976	543.985876	10.249575
5.461047	537.016112	10.254579
5.358241	555.241104	10.259584
5.523960	540.878951	10.264589
5.602644	545.493050	10.269594
5.406485	557.907821	10.274599
5.897250	551.714270	10.279603
5.401201	552.203369	10.284608
5.730911	554.426259	10.289613
5.507704	563.647369	10.294618
5.697978	568.527523	10.299623
5.955646	573.146201	10.304627
5.566155	592.569687	10.309632
5.818391	580.877610	10.314637
5.914508	586.075555	10.319642
5.928091	588.703674	10.324647
6.128263	582.269457	10.329651
6.074542	593.614469	10.334656
6.449207	580.491525	10.339661
6.269682	592.244521	10.344666
6.559610	598.297788	10.349671
6.617423	592.815075	10.354675
6.590147	595.995326	10.359680
6.850009	591.156887	10.364685
6.771190	593.897514	10.369690
6.443952	596.304031	10.374695
6.784116	585.145117	10.379699
6.546115	608.188718	10.384704
6.726245	594.081252	10.389709
6.437172	603.699237	10.394714
6.740657	602.710980	10.399719
6.708604	622.946382	10.404723
6.848226	629.720633	10.409728
7.231224	618.701516	10.414733
6.994214	639.015359	10.419738
6.989101	634.384743	10.424743
7.571979	629.754966	10.429747
7.118322	631.043114	10.434752
7.054699	625.483564	10.439757
6.916068	634.177154	10.444762
7.018605	639.465556	10.449767
7.181607	639.039009	10.454771
6.853679	636.353762	10.459776
7.087900	640.916278	10.464781
7.036894	649.371978	10.469786
7.406140	643.238769	10.474791
7.199443	663.025849	10.479795
7.415488	675.494826	10.484800
7.728271	680.055863	10.489805
7.562934	686.262199	10.494810
7.817991	678.890375	10.499815
8.033809	683.113647	10.504819
8.137488	679.310898	10.509824
8.459023	680.432840	10.514829
8.005093	658.813034	10.519834
8.019683	663.598240	10.524839
8.054723	655.805787	10.529843
7.813623	656.544382	10.534848
8.204577	651.882131	10.539853
7.828191	664.937584	10.544858
8.033103	667.279742	10.549863
8.304075	678.744921	10.554867
7.950588	690.238740	10.559872
8.625798	689.293693	10.564877
8.455662	689.270355	10.569882
8.309614	690.791718	10.574887
8.384584	688.764436	10.579891
8.408678	690.194010	10.584896
8.554574	693.600549	10.589901
8.646860	688.653189	10.594906
8.727500	696.442957	10.599911
8.876146	689.546986	10.604915
8.757798	690.821084	10.609920
8.796593	692.065390	10.614925
8.792245	691.184569	10.619930
8.712723	687.623922	10.624935
9.027762	696.136386	10.629939
8.310641	692.874543	10.634944
8.902473	685.731275	10.639949
8.722431	704.397696	10.644954
8.705265	699.622327	10.649959
8.870325	699.763145	10.654963
8.610089	690.224798	10.659968
8.755458	709.156289	10.664973
9.027540	716.488188	10.669978
9.160740	721.951500	10.674983
9.219797	731.764779	10.679987
9.487068	731.662218	10.684992
9.449237	731.199892	10.689997
9.323982	730.666354	10.695002
9.253746	728.990227	10.700007
9.536176	731.689034	10.705011
9.479030	735.949548	10.710016
9.562253	745.962407	10.715021
9.589402	746.445339	10.720026
9.648218	735.761684	10.725031
9.841598	738.399002	10.730035
9.845239	734.005075	10.735040
9.751806	734.341660	10.740045
9.783766	736.124793	10.745050
9.637966	740.948220	10.750055
9.908180	738.842485	10.755059
9.855394	736.496531	10.760064
10.267495	740.299013	10.765069
10.038826	739.376696	10.770074
9.979645	744.265156	10.775079
10.279523	749.982589	10.780083
10.011445	764.593061	10.785088
10.161452	760.546363	10.790093
10.331983	767.126516	10.795098
10.115627	763.499365	10.800103
10.632606	766.701661	10.805107
10.332353	772.383930	10.810112
10.328765	767.896530	10.815117
10.378515	768.495705	10.820122
10.627174	769.600892	10.825127
10.978770	768.135025	10.830131
10.444997	765.621352	10.835136
10.623071	758.318536	10.840141
10.679024	774.063194	10.845146
10.427796	772.958394	10.850151
10.793340	767.540076	10.855155
10.744630	776.197332	10.860160
10.750660	773.091370	10.865165
10.523122	769.226306	10.870170
10.489292	778.653890	10.875175
10.963006	790.962024	10.880179
10.932236	812.933697	10.885184
10.815617	804.222340	10.890189
11.356903	803.733882	10.895194
11.376976	805.119954	10.900199
11.457218	812.288534	10.905203
11.338737	811.306061	10.910208
11.414825	811.268684	10.915213
11.457010	807.377939	10.920218
11.533317	808.236230	10.925223
11.674233	793.423624	10.930227
11.343009	806.759004	10.935232
11.603972	817.446881	10.940237
11.700241	805.241761	10.945242
11.435002	803.273453	10.950247
11.637944	815.971720	10.955251
11.178853	808.289530	10.960256
11.571569	798.519242	10.965261
11.509674	812.428256	10.970266
11.457401	826.483981	10.975271
12.177331	827.760015	10.980275
11.751491	834.734931	10.985280
12.043221	827.033911	10.990285
12.317785	833.070804	10.995290
12.319025	829.858361	11.000295
12.259135	833.365562	11.005299
11.960776	838.626511	11.010304
12.382926	827.214642	11.015309
12.258736	832.425734	11.020314
12.323007	835.567783	11.025319
12.699017	824.117543	11.030323
12.425762	836.746696	11.035328
12.357464	843.175741	11.040333
12.183056	843.481087	11.045338
12.262387	834.850424	11.050343
12.556237	836.210182	11.055347
12.556872	837.596204	11.060352
12.721556	830.951495	11.065357
12.442269	829.403313	11.070362
12.537694	841.792323	11.075367
13.009758	835.749869	11.080371
12.839416	836.029335	11.085376
12.724284	829.970146	11.090381
12.791216	840.126016	11.095386
12.577484	844.790002	11.100391
12.767300	862.651744	11.105395
12.515182	877.616174	11.110400
13.182681	866.302339	11.115405
13.119045	866.894371	11.120410
13.235882	870.158930	11.125415
13.467324	876.496031	11.130419
13.395854	870.549709	11.135424
13.530465	867.746494	11.140429
13.427375	880.257083	11.145434
13.511628	866.623536	11.150439
13.714715	872.971465	11.155443
13.522832	876.435072	11.160448
13.893328	864.752292	11.165453
13.885941	870.930362	11.170458
13.679630	876.619766	11.175463
13.889740	857.599801	11.180467
13.785030	871.337505	11.185472
13.977562	869.133754	11.190477
13.638754	858.362037	11.195482
13.520758	861.550507	11.200487
13.705185	871.626160	11.205491
13.639128	870.977520	11.210496
13.711609	870.272092	11.215501
13.297971	875.931484	11.220506
13.442720	876.176469	11.225511
14.208774	883.670946	11.230515
14.103661	894.336840	11.235520
14.266108	899.674130	11.240525
14.558945	896.440399	11.245530
14.725273	882.399509	11.250535
14.452344	874.892596	11.255539
14.520182	871.404596	11.260544
14.607611	859.096762	11.265549
14.348288	872.699854	11.270554
14.378206	870.216109	11.275559
14.495438	864.293311	11.280563
14.516539	876.396161	11.285568
14.867404	879.735363	11.290573
14.851764	877.555349	11.295578
14.605520	870.115146	11.300583
14.773320	868.569773	11.305587
14.578976	884.349739	11.310592
14.651162	895.137167	11.315597
15.111377	899.695263	11.320602
15.134946	897.013830	11.325607
15.344662	893.321848	11.330611
15.289718	888.106165	11.335616
15.178811	868.277945	11.340621
14.965890	871.707060	11.345626
15.287111	863.512463	11.350631
15.131369	872.346118	11.355635
15.169653	895.229417	11.360640
15.497535	883.080333	11.365645
15.685047	888.486161	11.370650
14.926413	889.160649	11.375655
15.430344	881.482528	11.380659
15.419042	894.819005	11.385664
15.876521	887.574065	11.390669
15.592938	890.069861	11.395674
15.787601	900.594909	11.400679
15.909951	884.465264	11.405683
15.586814	878.167992	11.410688
15.793937	880.859915	11.415693
16.026204	898.226078	11.420698
16.110312	889.723931	11.425703
15.711470	868.044561	11.430707
15.814557	876.193545	11.435712
16.026805	874.801932	11.440717
15.736672	893.358421	11.445722
15.898639	893.290001	11.450727
16.144452	886.449402	11.455731
15.960590	897.389631	11.460736
16.109461	881.575880	11.465741
16.282081	898.502126	11.470746
16.086760	897.352129	11.475751
16.080096	892.616022	11.480755
15.999954	892.444289	11.485760
16.214543	888.732608	11.490765
15.990096	898.578599	11.495770
16.081373	896.394147	11.500775
16.570564	913.509619	11.505779
16.230856	932.316915	11.510784
16.575156	919.840329	11.515789
16.687876	925.666530	11.520794
16.583763	929.904629	11.525799
16.447953	928.172705	11.530803
16.808527	932.764049	11.535808
16.894456	931.320036	11.540813
16.998442	931.972069	11.545818
16.943683	926.474068	11.550823
17.088276	924.506613	11.555827
17.018020	925.307860	11.560832
16.914366	925.169838	11.565837
17.283648	925.159819	11.570842
17.138890	923.484515	11.575847
17.162785	932.581294	11.580851
17.028938	927.873344	11.585856
17.286355	918.181324	11.590861
17.327716	922.903999	11.595866
17.441152	926.419850	11.600871
17.717924	920.537817	11.605875
17.546244	931.425666	11.610880
17.730673	921.873018	11.615885
17.621701	921.199680	11.620890
17.590243	925.804659	11.625895
17.893969	930.628997	11.630899
17.552668	932.208332	11.635904
17.767037	925.153533	11.640909
17.659277	932.462543	11.645914
17.402789	927.034561	11.650919
17.696967	926.688012	11.655923
17.581932	938.883589	11.660928
17.826084	949.291971	11.665933
18.220485	960.316644	11.670938
18.232450	948.217889	11.675943
18.319950	945.624023	11.680947
18.043004	934.374027	11.685952
18.392428	932.548946	11.690957
18.326971	927.304962	11.695962
17.620300	925.312420	11.700967
18.180096	938.546818	11.705971
18.170078	947.483435	11.710976
18.399067	950.187654	11.715981
18.436207	957.624955	11.720986
18.460631	947.512757	11.725991
18.660823	947.212737	11.730995
18.618849	956.706390	11.736000
18.909569	946.876576	11.741005
19.076214	942.180622	11.746010
18.691243	957.152129	11.751015
18.752533	942.725808	11.756019
18.297440	953.493293	11.761024
18.943437	944.122485	11.766029
18.554532	950.326741	11.771034
18.644789	952.146336	11.776039
19.262377	949.004304	11.781043
19.273706	944.006690	11.786048
19.095719	946.039376	11.791053
18.931923	951.114901	11.796058
18.731343	945.652763	11.801063
19.281458	957.609812	11.806067
19.052129	952.753078	11.811072
19.047539	953.466583	11.816077
18.855048	956.611761	11.821082
18.953507	957.048634	11.826087
19.101093	971.413249	11.831091
19.098612	983.657146	11.836096
19.549561	983.870646	11.841101
19.299212	994.908284	11.846106
19.509013	993.551743	11.851111
19.637910	983.460705	11.856115
19.848588	984.458427	11.861120
19.826953	982.769788	11.866125
19.868070	982.955609	11.871130
19.868960	982.728373	11.876135
20.053851	985.980529	11.881139
19.456270	985.590118	11.886144
20.102467	980.833441	11.891149
19.919865	987.402205	11.896154
19.577153	978.840341	11.901159
20.286109	975.948662	11.906163
20.048257	985.230722	11.911168
20.250383	982.005131	11.916173
20.048844	979.220812	11.921178
20.246539	975.344645	11.926183
20.317356	983.301716	11.931187
20.178032	978.296577	11.936192
20.110471	982.375897	11.941197
20.005516	978.068601	11.946202
20.155070	977.180565	11.951207
20.461317	985.557409	11.956211
20.639175	997.010885	11.961216
20.712853	987.133656	11.966221
20.836255	1002.553992	11.971226
21.075782	977.024211	11.976231
21.108052	970.979300	11.981235
20.810835	973.251779	11.986240
20.897852	973.846596	11.991245
20.926762	969.210447	11.996250
20.975830	967.166757	12.001255
21.084832	968.814630	12.006259
20.656814	970.455107	12.011264
21.067758	960.109369	12.016269
21.042329	966.623095	12.021274
21.106036	975.536933	12.026279
21.093929	972.911639	12.031283
20.904384	972.815700	12.036288
21.148544	980.767203	12.041293
21.185289	969.169105	12.046298
20.857170	975.308484	12.051303
21.085309	965.807183	12.056307
21.139099	973.790619	12.061312
21.116475	973.600250	12.066317
21.195689	977.427502	12.071322
20.903931	962.838268	12.076327
21.032183	978.271997	12.081331
20.870228	973.191621	12.086336
21.060208	972.416987	12.091341
20.855204	981.017290	12.096346
20.988636	975.102902	12.101351
20.896152	978.899189	12.106355
21.006609	982.022865	12.111360
20.873830	974.463586	12.116365
20.931535	976.515457	12.121370
20.740635	987.064213	12.126375
21.119429	980.022590	12.131379
21.095365	991.831541	12.136384
21.043372	993.186546	12.141389
21.201345	989.360866	12.146394
20.886339	987.905095	12.151399
21.149112	973.791965	12.156403
21.060064	990.790013	12.161408
21.143706	971.952494	12.166413
20.935196	987.093009	12.171418
21.035797	978.149784	12.176423
21.198567	984.239264	12.181427
20.904251	975.980344	12.186432
21.019833	968.884509	12.191437
21.091302	983.218697	12.196442
21.284182	978.050191	12.201447
21.390522	986.186103	12.206451
21.004667	976.713329	12.211456
21.285342	973.520946	12.216461
21.265260	980.524259	12.221466
21.151382	983.598558	12.226471
21.185063	979.097263	12.231475
21.239258	984.013454	12.236480
21.139197	985.789288	12.241485
21.152055	985.837689	12.246490
21.114348	979.045418	12.251495
21.191589	983.407575	12.256499
20.884111	993.862963	12.261504
21.258189	978.013190	12.266509
21.090641	980.179834	12.271514
21.166840	986.119118	12.276519
21.420463	988.324250	12.281523
20.896794	974.117345	12.286528
21.128304	970.554332	12.291533
21.196702	968.677871	12.296538
21.055792	970.983769	12.301543
21.006353	951.285980	12.306547
20.949075	963.101782	12.311552
21.101029	952.442537	12.316557
20.976694	955.406534	12.321562
20.863875	953.194698	12.326567
21.332781	970.392322	12.331571
21.126218	975.217632	12.336576
21.120579	957.883019	12.341581
21.175455	951.949629	12.346586
21.134461	953.820119	12.351591
21.304642	959.725480	12.356595
20.808217	954.558103	12.361600
21.326559	950.851579	12.366605
21.179732	955.985901	12.371610
21.044977	950.191564	12.376615
21.404277	961.642884	12.381619
21.300393	955.711157	12.386624
21.260204	955.134082	12.391629
21.543762	947.574650	12.396634
21.320465	959.344386	12.401639
21.303005	942.738654	12.406643
20.932503	941.914636	12.411648
21.176063	918.866442	12.416653
21.037931	931.688593	12.421658
20.757384	929.568166	12.426663
20.843948	923.484654	12.431667
20.935579	950.224647	12.436672
21.181404	955.652741	12.441677
21.100821	961.052467	12.446682
21.094237	958.650223	12.451687
21.157965	945.440921	12.456691
20.900551	936.496471	12.461696
21.001586	951.442503	12.466701
21.027262	945.568966	12.471706
20.922618	949.379800	12.476711
21.333138	947.041925	12.481715
20.991333	943.236037	12.486720
21.041017	925.533094	12.491725
20.803468	945.398020	12.496730
21.259398	946.664132	12.501735
21.283292	952.083463	12.506739
20.824327	947.838942	12.511744
20.972911	931.241435	12.516749
20.879538	944.974247	12.521754
21.001691	959.831764	12.526759
21.274627	964.683101	12.531763
20.853662	948.272601	12.536768
20.985938	952.701666	12.541773
21.221306	961.701659	12.546778
21.244350	965.952605	12.551783
21.085015	942.175419	12.556787
20.503057	940.197677	12.561792
20.708916	959.542475	12.566797
20.857095	959.512524	12.571802
21.074976	977.825676	12.576807
21.370436	968.185903	12.581811
20.998682	977.848860	12.586816
21.385366	962.534836	12.591821
21.355677	976.730610	12.596826
21.062530	963.018387	12.601831
21.365989	946.167504	12.606835
20.756923	952.124597	12.611840
20.927529	937.750234	12.616845
20.840785	952.484939	12.621850
21.060691	951.776497	12.626855
21.109791	961.957375	12.631859
21.195396	947.509825	12.636864
21.138469	958.794133	12.641869
21.198799	944.596623	12.646874
20.863243	948.504207	12.651879
21.004339	948.159994	12.656883
20.841665	956.441295	12.661888
20.868072	953.142809	12.666893
21.216210	965.549971	12.671898
20.927951	964.067859	12.676903
21.358429	962.173078	12.681907
21.019995	960.621698	12.686912
21.364622	941.532860	12.691917
21.006351	945.492952	12.696922
21.290645	960.135376	12.701927
21.375550	946.747654	12.706931
21.031662	952.233524	12.711936
21.150951	940.750018	12.716941
21.216794	955.017267	12.721946
21.185725	951.668024	12.726951
21.451391	940.534913	12.731955
21.089488	952.452905	12.736960
21.463510	942.824274	12.741965
21.256617	955.513910	12.746970
20.928222	957.162152	12.751975
21.427147	946.058068	12.756979
20.654412	948.409533	12.761984
21.048915	945.793514	12.766989
21.071069	948.939151	12.771994
21.007019	950.152573	12.776999
21.301863	951.263025	12.782003
20.837251	955.575971	12.787008
21.145530	952.286149	12.792013
21.139412	945.495163	12.797018
20.827257	931.128411	12.802023
21.229076	946.882755	12.807027
20.936474	939.708528	12.812032
20.797603	931.560462	12.817037
20.901647	946.856092	12.822042
20.715333	955.365090	12.827047
20.930472	955.742354	12.832051
21.022789	960.579917	12.837056
21.023811	956.470192	12.842061
21.009051	955.409666	12.847066
20.891292	959.455984	12.852071
20.891927	965.752664	12.857075
21.003714	954.588889	12.862080
21.274996	964.400021	12.867085
21.263264	951.388829	12.872090
21.134957	962.824874	12.877095
21.186635	958.055786	12.882099
21.155250	952.730666	12.887104
21.056374	955.165475	12.892109
21.006408	950.992921	12.897114
20.999534	964.984770	12.902119
21.204903	948.256762	12.907123
20.955934	963.334319	12.912128
21.108982	962.062526	12.917133
21.365291	960.198675	12.922138
21.127762	951.806133	12.927143
21.265183	926.347919	12.932147
20.998996	933.150762	12.937152
20.988000	930.069559	12.942157
21.255402	919.988015	12.947162
21.058154	929.109022	12.952167
21.244893	925.881167	12.957171
21.264027	927.466097	12.962176
21.350129	924.538143	12.967181
21.304475	922.422834	12.972186
21.077464	933.685362	12.977191
21.248680	925.749620	12.982195
21.009219	938.693593	12.987200
21.070814	929.944276	12.992205
21.202390	935.433160	12.997210
21.335700	921.113647	13.002215
21.305884	928.138988	13.007219
21.288402	931.202633	13.012224
21.362907	918.846346	13.017229
21.216419	912.421538	13.022234
20.926119	907.894663	13.027239
21.176809	897.361638	13.032243
21.159938	904.408558	13.037248
20.856863	889.784933	13.042253
20.831299	898.958965	13.047258
20.852070	907.881186	13.052263
21.593514	893.821104	13.057267
21.132122	904.299398	13.062272
21.346038	904.074460	13.067277
21.052125	912.386127	13.072282
20.740036	904.057544	13.077287
20.946232	902.029805	13.082291
20.603458	910.738770	13.087296
21.011419	904.913092	13.092301
21.112192	903.074054	13.097306
20.806307	898.844557	13.102311
20.829334	901.893851	13.107315
20.784895	924.938625	13.112320
20.907157	919.994289	13.117325
21.400099	931.454234	13.122330
21.167742	934.862808	13.127335
21.357753	919.313690	13.132339
20.682596	919.864478	13.137344
21.016133	918.803601	13.142349
21.220655	927.903110	13.147354
21.009383	927.591440	13.152359
20.890054	924.197932	13.157363
20.645216	929.336837	13.162368
20.943368	936.480188	13.167373
20.907244	940.789449	13.172378
20.947972	940.338241	13.177383
21.601660	935.288648	13.182387
20.908509	949.601243	13.187392
21.431195	945.449326	13.192397
21.226141	936.942804	13.197402
20.994251	926.142944	13.202407
21.361019	910.324373	13.207411
20.862084	910.186313	13.212416
21.039951	909.355267	13.217421
21.087673	909.352376	13.222426
20.852357	920.925302	13.227431
21.051033	903.293241	13.232435
20.878628	928.772742	13.237440
20.914312	906.508350	13.242445
21.045714	933.125275	13.247450
20.894361	930.389731	13.252455
21.047401	943.857740	13.257459
20.841986	943.262860	13.262464
20.961247	934.274108	13.267469
20.999962	933.190863	13.272474
21.020293	935.417423	13.277479
21.433232	942.913056	13.282483
21.089126	941.365737	13.287488
20.940007	945.063814	13.292493
21.173735	939.366834	13.297498
20.972697	945.640475	13.302503
21.073357	941.518018	13.307507
20.990337	949.382910	13.312512
21.034799	940.819246	13.317517
21.093027	943.306269	13.322522
20.769436	945.040476	13.327527
21.115759	944.242487	13.332531
20.875715	942.115598	13.337536
20.991717	936.839518	13.342541
21.245982	940.525302	13.347546
21.162984	947.130202	13.352551
21.339799	946.665175	13.357555
21.071219	935.002258	13.362560
21.145802	929.892058	13.367565
21.032928	922.853180	13.372570
21.057388	922.505492	13.377575
20.973094	913.891415	13.382579
20.889718	918.615059	13.387584
20.721410	921.932991	13.392589
20.873059	937.508025	13.397594
20.877072	946.048165	13.402599
21.036380	942.655946	13.407603
21.024176	945.086393	13.412608
20.813898	942.041700	13.417613
21.004686	938.814773	13.422618
20.774607	951.044478	13.427623
21.438058	947.155541	13.432627
21.034697	944.570572	13.437632
21.207772	938.728724	13.442637
21.270058	946.113124	13.447642
21.351860	942.335873	13.452647
21.248377	950.524152	13.457651
20.932735	929.167312	13.462656
20.878659	923.860014	13.467661
21.088192	927.822587	13.472666
20.831659	943.316068	13.477671
21.125823	947.911701	13.482675
20.797001	948.981268	13.487680
20.712125	952.293786	13.492685
20.743393	957.584209	13.497690
21.008470	951.024361	13.502695
20.963853	952.248876	13.507699
20.930573	953.476313	13.512704
20.927128	947.545919	13.517709
21.098189	942.298903	13.522714
21.029246	955.835441	13.527719
21.243762	939.974886	13.532723
21.041492	956.705523	13.537728
21.285286	941.893704	13.542733
21.260826	960.439449	13.547738
21.148294	949.201066	13.552743
21.375293	954.928629	13.557747
21.097382	963.538972	13.562752
21.177649	951.042967	13.567757
21.247673	950.385236	13.572762
20.856815	942.357775	13.577767
20.624128	936.448175	13.582771
21.021508	952.789860	13.587776
20.861790	948.002450	13.592781
20.986626	948.976013	13.597786
20.646905	953.059305	13.602791
21.161543	948.828246	13.607795
20.836834	966.981912	13.612800
21.014628	955.216250	13.617805
20.930911	951.864365	13.622810
20.818061	963.200173	13.627815
20.729868	950.675841	13.632819
20.801711	957.079432	13.637824
21.207261	962.270743	13.642829
21.046027	963.461817	13.647834
20.952205	957.011243	13.652839
21.281496	962.385027	13.657843
21.024672	964.818219	13.662848
21.149141	955.303497	13.667853
21.319496	959.718606	13.672858
21.111948	958.673056	13.677863
21.350449	949.427157	13.682867
21.029897	955.145850	13.687872
21.315026	961.159036	13.692877
21.328187	954.612554	13.697882
21.027331	964.852399	13.702887
20.882157	958.890986	13.707891
21.290384	957.572189	13.712896
20.963482	968.003849	13.717901
21.112683	961.516093	13.722906
21.085813	967.758812	13.727911
21.239347	965.752079	13.732915
21.120812	959.928343	13.737920
21.146182	963.109741	13.742925
21.008554	942.033576	13.747930
20.666907	941.670158	13.752935
21.195569	944.418047	13.757939
21.182847	962.359525	13.762944
21.216241	953.384455	13.767949
21.009393	936.551890	13.772954
20.853613	950.341969	13.777959
20.898999	937.922501	13.782963
20.892648	948.667301	13.787968
21.268779	950.570615	13.792973
20.865344	962.826399	13.797978
20.887748	969.274151	13.802983
21.315228	955.965827	13.807987
20.951775	967.778423	13.812992
21.079910	967.436277	13.817997
21.113162	963.584762	13.823002
21.135602	966.296694	13.828007
21.313935	957.396278	13.833011
20.771215	943.827955	13.838016
20.998525	934.355192	13.843021
20.875498	943.927996	13.848026
20.891965	948.326643	13.853031
21.238502	948.433792	13.858035
21.394228	961.513457	13.863040
21.183091	957.314565	13.868045
21.052419	945.334755	13.873050
21.021634	939.101217	13.878055
21.278157	933.230293	13.883059
20.921916	939.024058	13.888064
21.016238	916.277213	13.893069
20.898152	930.636849	13.898074
20.482368	932.150792	13.903079
21.207110	945.849325	13.908083
21.281505	961.886139	13.913088
20.834586	950.436155	13.918093
21.050774	944.314615	13.923098
20.916488	963.584355	13.928103
21.089057	958.507404	13.933107
20.998306	960.904649	13.938112
21.281894	956.980096	13.943117
21.077770	940.927684	13.948122
20.862131	949.687361	13.953127
21.404668	946.140983	13.958131
20.991097	943.071941	13.963136
21.035623	944.228622	13.968141
20.858191	941.733779	13.973146
20.958380	938.325759	13.978151
20.940111	938.901096	13.983155
20.873913	961.777510	13.988160
21.258252	964.743963	13.993165
21.237449	949.521748	13.998170
20.912311	945.008303	14.003175
21.041312	934.762740	14.008179
21.049615	945.394814	14.013184
21.128476	938.710128	14.018189
21.324306	938.454841	14.023207
20.849195	944.545495	14.028224
21.096915	929.000013	14.033242
21.045726	941.574319	14.038259
20.911612	945.137941	14.043277
21.320716	943.364480	14.048295
21.143541	957.085112	14.053312
21.411763	947.202051	14.058330
21.071530	942.344031	14.063347
21.077165	945.940418	14.068365
21.086485	951.299478	14.073383
21.049873	960.149914	14.078400
21.206705	959.901534	14.083418
20.962777	960.918791	14.088435
21.354117	972.595184	14.093453
21.338218	958.630044	14.098471
21.431488	972.670907	14.103488
21.727840	966.684228	14.108506
21.459929	969.762710	14.113523
21.468886	970.775814	14.118541
21.232870	952.460439	14.123559
21.229717	968.147808	14.128576
21.298474	961.796330	14.133594
20.933657	980.721866	14.138611
21.299434	968.698194	14.143629
21.388110	978.681623	14.148647
21.193537	971.022557	14.153664
21.498007	968.649190	14.158682
21.487635	972.016915	14.163699
21.383746	971.404298	14.168717
21.490178	978.968866	14.173735
21.412595	978.896289	14.178752
21.648521	976.324651	14.183770
21.408007	975.842356	14.188787
21.458495	981.256205	14.193805
21.604005	982.249105	14.198823
21.523579	1002.397101	14.203840
21.860296	998.906518	14.208858
21.884147	996.938103	14.213875
21.699267	1013.763425	14.218893
21.965166	1006.177187	14.223911
21.788943	1006.213145	14.228928
21.760993	1000.715450	14.233946
21.772544	1011.261729	14.238963
21.751659	1004.852173	14.243981
21.860454	1005.163556	14.248999
21.667082	1010.372501	14.254016
22.085111	1004.872889	14.259034
21.957718	1010.492860	14.264051
21.997837	1003.463275	14.269069
22.159721	1006.578606	14.274087
21.991794	1017.302943	14.279104
22.303731	1002.395192	14.284122
21.878214	987.199249	14.289139
21.608118	989.916307	14.294157
21.812791	996.751103	14.299175
21.771096	1008.405356	14.304192
22.037950	1009.164986	14.309210
21.812857	1003.678282	14.314227
22.200220	1007.916910	14.319245
22.188934	1007.773989	14.324263
21.940912	1007.646801	14.329280
22.023558	1003.509362	14.334298
21.944297	1008.426417	14.339315
21.784669	1002.905678	14.344333
21.879692	1006.945551	14.349351
21.765482	1004.833994	14.354368
22.290005	1024.048738	14.359386
22.332046	1039.813916	14.364403
22.561931	1030.485870	14.369421
22.856411	1034.684266	14.374439
22.598573	1020.048254	14.379456
22.672485	1010.782846	14.384474
22.497542	1006.430097	14.389491
22.190134	1005.694215	14.394509
22.335148	1009.888128	14.399527
22.373318	999.690955	14.404544
22.330491	1002.043026	14.409562
22.424181	1004.431524	14.414579
22.427288	1005.738130	14.419597
22.512662	996.244400	14.424615
22.171930	1006.827984	14.429632
22.576611	998.294729	14.434650
22.432550	1015.703395	14.439667
22.493736	1028.168624	14.444685
22.934435	1015.255264	14.449703
22.650746	1014.081467	14.454720
22.794133	1001.154190	14.459738
22.745002	1009.385342	14.464755
22.376508	1008.168444	14.469773
22.700788	1000.266176	14.474791
22.696354	1022.792949	14.479808
23.083823	1018.308033	14.484826
22.788159	1007.121235	14.489843
22.832227	1005.126000	14.494861
22.953263	1000.356409	14.499879
22.683429	1005.121395	14.504896
22.804880	999.724136	14.509914
22.826399	987.824560	14.514931
22.671822	1006.475941	14.519949
23.058098	1008.695089	14.524967
22.762871	1007.862887	14.529984
23.046317	1026.332758	14.535002
22.833206	1021.050192	14.540019
23.121545	1025.984129	14.545037
23.690931	1016.406903	14.550055
23.319785	1009.411445	14.555072
22.910516	1002.645427	14.560090
22.909907	1001.014376	14.565107
22.879877	1004.786343	14.570125
22.994987	993.082611	14.575143
22.911117	1012.328304	14.580160
23.232515	994.104868	14.585178
23.239429	993.315712	14.590195
22.796602	1004.343416	14.595213
23.288482	991.006659	14.600231
23.121718	1007.311588	14.605248
23.077483	1011.796791	14.610266
23.149604	1030.951567	14.615283
23.182688	1030.908529	14.620301
23.433783	1026.171669	14.625319
23.030865	1037.937034	14.630336
23.254290	1028.603727	14.635354
23.484641	1029.589392	14.640371
23.244878	1040.204085	14.645389
23.473525	1036.427151	14.650407
23.440009	1029.566590	14.655424
23.445958	1027.792925	14.660442
23.506991	1028.247198	14.665459
23.322939	1032.797175	14.670477
23.646072	1020.516008	14.675495
23.438900	1029.492783	14.680512
23.654937	1032.580609	14.685530
23.873044	1014.169138	14.690547
23.369821	1040.803787	14.695565
23.660480	1029.984337	14.700583
23.494815	1040.950563	14.705600
23.573748	1020.406348	14.710618
23.532697	1033.532792	14.715635
23.477117	1034.395752	14.720653
23.672323	1026.199466	14.725671
23.929334	1030.861564	14.730688
23.658457	1029.858746	14.735706
23.954361	1029.454486	14.740723
23.871585	1033.574628	14.745741
23.988224	1028.126219	14.750759
23.756604	1034.970841	14.755776
23.708136	1028.730832	14.760794
23.920100	1025.747751	14.765811
23.873962	1028.219898	14.770829
23.979692	1020.936034	14.775847
23.828539	1033.174023	14.780864
23.636453	1032.757930	14.785882
24.278165	1024.998496	14.790899
23.917238	1027.000202	14.795917
24.006870	1028.193916	14.800935
23.821794	1028.173086	14.805952
23.696549	1028.087662	14.810970
23.755711	1022.808861	14.815987
23.790910	1041.596753	14.821005
24.289256	1031.934897	14.826023
23.843233	1039.228971	14.831040
24.036435	1029.173784	14.836058
24.260663	1028.420752	14.841075
23.830368	1038.817305	14.846093
24.213539	1028.607560	14.851111
24.211188	1033.287427	14.856128
24.240805	1029.929180	14.861146
24.290184	1026.007814	14.866163
23.998514	1040.593026	14.871181
24.035365	1047.084969	14.876199
24.293820	1053.233275	14.881216
24.619363	1065.459758	14.886234
24.574960	1049.386610	14.891251
24.292639	1059.600712	14.896269
24.533202	1045.116412	14.901287
24.249790	1037.395978	14.906304
24.370061	1058.271776	14.911322
24.552921	1063.886331	14.916339
24.249977	1062.501680	14.921357
24.689521	1063.589258	14.926375
24.690015	1054.165653	14.931392
24.621982	1062.879598	14.936410
24.516967	1041.933701	14.941427
24.484337	1064.336054	14.946445
24.533455	1055.912951	14.951463
24.837524	1065.176284	14.956480
24.877343	1059.826626	14.961498
24.666663	1047.183852	14.966515
24.665424	1039.160453	14.971533
24.942424	1052.712794	14.976551
24.664503	1028.102791	14.981568
24.360496	1039.345896	14.986586
24.894170	1048.383848	14.991603
24.708951	1060.820765	14.996621
24.603437	1056.546586	15.001639
24.902514	1048.890545	15.006656
24.869364	1048.820319	15.011674
25.399456	1058.393650	15.016691
24.961937	1049.124841	15.021709
25.006432	1061.172783	15.026727
25.107285	1060.057199	15.031744
24.903595	1052.736154	15.036762
24.858068	1048.161417	15.041779
24.789451	1060.206950	15.046797
24.806318	1052.907356	15.051815
24.754134	1052.297500	15.056832
24.973952	1061.901440	15.061850
25.236981	1053.776116	15.066867
25.225857	1053.386215	15.071885
25.494541	1041.590316	15.076903
25.404992	1055.971859	15.081920
25.039446	1064.967622	15.086938
25.392222	1050.624288	15.091955
25.393451	1057.225730	15.096973
25.466327	1053.204660	15.101991
24.989594	1069.074625	15.107008
25.235742	1057.147034	15.112026
25.506484	1055.699205	15.117043
25.051596	1064.179133	15.122061
25.469012	1053.503036	15.127079
25.631973	1063.562761	15.132096
25.291141	1053.474754	15.137114
25.387943	1062.168703	15.142131
25.608132	1055.297556	15.147149
25.727794	1057.512043	15.152167
25.447855	1057.990809	15.157184
25.114871	1055.599546	15.162202
25.487502	1055.244394	15.167219
25.216535	1060.492472	15.172237
25.430003	1054.010915	15.177255
25.677521	1055.923454	15.182272
25.561700	1057.470817	15.187290
25.637357	1052.908210	15.192307
25.568675	1057.708770	15.197325
25.548494	1058.798882	15.202343
25.313520	1058.479286	15.207360
25.451036	1052.005124	15.212378
25.936863	1042.957133	15.217395
25.870931	1050.934598	15.222413
26.122957	1042.345443	15.227431
26.306238	1042.429454	15.232448
25.992909	1045.755855	15.237466
26.272794	1050.044669	15.242483
26.309853	1047.652591	15.247501
26.245361	1052.222831	15.252519
26.195395	1042.130914	15.257536
26.126403	1047.400257	15.262554
26.115857	1044.910384	15.267571
25.921054	1040.035429	15.272589
26.097785	1031.681646	15.277607
26.015066	1036.937445	15.282624
25.997936	1039.527657	15.287642
25.871885	1046.780144	15.292659
25.921092	1044.345233	15.297677
26.110471	1051.103846	15.302695
26.351536	1043.208535	15.307712
26.124628	1053.925002	15.312730
26.205325	1046.624670	15.317747
26.293177	1048.068767	15.322765
25.880420	1046.572649	15.327783
26.145099	1039.623631	15.332800
25.814083	1051.385405	15.337818
26.149019	1046.937172	15.342835
26.246475	1053.417879	15.347853
26.156611	1043.791624	15.352871
26.320520	1045.071016	15.357888
26.026077	1051.611076	15.362906
26.448368	1049.467432	15.367923
26.391031	1065.232757	15.372941
26.411319	1061.319167	15.377959
26.685280	1063.567246	15.382976
26.446837	1062.381510	15.387994
26.378823	1061.270836	15.393011
26.827119	1057.677506	15.398029
26.558841	1057.624330	15.403047
26.543027	1054.547014	15.408064
26.722049	1062.309251	15.413082
26.556313	1057.464259	15.418099
26.698877	1064.153271	15.423117
26.507341	1061.673384	15.428135
26.653589	1050.538765	15.433152
26.403477	1064.584146	15.438170
26.639027	1056.475786	15.443187
26.930485	1066.491427	15.448205
26.321235	1059.112367	15.453223
26.341114	1063.162666	15.458240
26.472723	1060.742924	15.463258
27.089614	1078.370066	15.468275
26.954290	1081.309454	15.473293
27.055711	1101.368815	15.478311
27.149677	1082.533484	15.483328
26.847223	1079.173130	15.488346
26.851628	1074.840520	15.493363
26.881552	1078.362284	15.498381
27.096635	1089.025592	15.503399
27.135376	1084.085063	15.508416
26.971098	1088.046767	15.513434
26.938364	1087.345723	15.518451
27.190812	1095.259854	15.523469
26.943538	1092.760538	15.528487
26.975331	1092.226945	15.533504
27.082318	1089.164643	15.538522
27.231559	1093.082641	15.543539
27.526113	1092.288504	15.548557
27.253398	1089.162493	15.553575
27.416207	1088.438128	15.558592
27.419727	1089.118642	15.563610
27.802236	1084.824825	15.568627
27.120594	1091.637428	15.573645
27.181329	1096.219170	15.578663
27.479047	1089.406425	15.583680
27.225326	1084.433890	15.588698
27.210812	1085.507371	15.593715
27.374561	1088.255927	15.598733
27.417947	1081.173875	15.603751
27.634771	1096.544744	15.608768
27.662344	1097.509273	15.613786
27.661370	1084.188113	15.618803
27.805163	1091.465224	15.623821
27.434362	1098.619922	15.628839
27.857452	1086.703412	15.633856
27.585389	1104.623359	15.638874
27.758796	1103.757311	15.643891
28.060196	1112.179572	15.648909
27.896237	1100.966977	15.653927
27.861394	1088.769582	15.658944
27.568205	1089.731784	15.663962
27.899466	1096.980574	15.668979
28.238454	1104.764511	15.673997
28.000142	1098.477674	15.679015
27.872076	1092.866927	15.684032
27.985524	1084.911725	15.689050
27.896469	1086.300673	15.694067
27.802367	1089.214613	15.699085
28.236039	1089.423852	15.704103
28.213675	1088.925637	15.709120
27.685116	1082.921037	15.714138
27.999037	1096.854476	15.719155
28.372452	1101.444553	15.724173
28.396127	1100.970454	15.729191
28.395339	1094.711802	15.734208
27.904724	1082.631141	15.739226
28.066252	1077.729231	15.744243
28.499855	1095.182715	15.749261
28.502679	1110.384817	15.754279
28.287533	1100.827265	15.759296
28.038992	1095.347410	15.764314
28.303310	1090.175859	15.769331
28.559738	1098.183734	15.774349
28.164312	1114.489073	15.779367
28.461724	1115.489216	15.784384
28.502656	1118.247927	15.789402
28.222588	1116.464810	15.794419
28.372324	1112.289901	15.799437
28.301305	1110.835225	15.804455
28.637891	1108.793326	15.809472
28.458720	1114.506534	15.814490
28.561194	1112.162212	15.819507
28.704972	1110.895067	15.824525
28.756785	1115.530145	15.829543
28.878019	1109.245735	15.834560
28.945651	1113.173608	15.839578
29.011176	1110.500141	15.844595
28.742362	1116.147425	15.849613
28.814415	1118.273564	15.854631
28.819739	1096.633622	15.859648
28.733769	1115.382734	15.864666
28.488114	1109.202451	15.869683
28.841112	1098.210994	15.874701
28.669937	1116.292609	15.879719
28.738116	1104.700087	15.884736
28.837836	1097.959811	15.889754
28.999169	1108.043422	15.894771
29.129178	1111.725403	15.899789
28.798303	1117.140351	15.904807
29.224785	1096.419484	15.909824
29.256096	1108.859661	15.914842
28.876065	1112.852634	15.919859
29.000352	1105.616103	15.924877
28.757886	1112.965836	15.929895
28.993870	1122.570385	15.934912
29.386193	1140.139040	15.939930
29.021198	1134.816162	15.944947
29.494558	1144.678585	15.949965
29.527687	1149.467657	15.954983
29.855535	1121.495433	15.960000
29.456717	1120.898384	15.965018
29.525283	1114.841012	15.970035
29.334340	1109.007490	15.975053
29.122722	1094.101347	15.980071
28.986091	1094.121553	15.985088
29.702752	1112.402903	15.990106
29.700960	1118.683973	15.995123
29.876680	1106.972057	16.000141
29.059322	1101.488536	16.005159
29.488164	1099.229015	16.010176
29.500747	1116.784273	16.015194
29.331368	1121.125882	16.020211
29.848149	1131.306972	16.025229
29.240107	1128.196678	16.030247
29.388372	1122.581176	16.035264
29.691167	1135.015830	16.040282
29.792323	1127.325248	16.045299
29.842020	1132.718833	16.050317
29.346413	1134.314187	16.055335
29.994163	1122.346090	16.060352
30.150362	1125.520554	16.065370
29.714754	1131.696216	16.070387
30.142192	1120.548159	16.075405
30.061370	1132.719962	16.080423
29.692902	1122.862818	16.085440
30.170131	1129.316027	16.090458
30.019924	1136.437136	16.095475
29.958602	1131.304919	16.100493
29.865383	1132.880144	16.105511
29.811085	1126.900560	16.110528
30.025379	1121.626869	16.115546
29.740613	1134.303083	16.120563
30.271558	1132.820042	16.125581
30.069861	1150.625009	16.130599
30.615987	1153.075080	16.135616
30.457628	1149.287480	16.140634
30.126193	1126.165994	16.145651
30.301711	1141.692930	16.150669
30.546210	1144.521423	16.155687
30.764306	1134.713866	16.160704
30.629063	1130.178577	16.165722
30.460219	1132.483129	16.170739
30.613395	1118.203020	16.175757
30.342282	1123.657200	16.180775
30.267379	1134.206347	16.185792
30.427508	1126.531528	16.190810
30.352271	1129.016197	16.195827
30.592977	1133.918445	16.200845
30.498893	1146.597293	16.205863
30.588916	1141.083875	16.210880
30.496265	1149.142731	16.215898
30.296303	1163.093696	16.220915
30.932913	1150.870961	16.225933
30.683537	1152.771526	16.230951
30.855665	1151.400760	16.235968
31.141625	1146.501005	16.240986
30.919305	1147.805824	16.246003
30.862028	1153.683643	16.251021
30.697233	1153.525878	16.256039
31.022271	1157.972684	16.261056
30.892650	1153.488399	16.266074
30.783497	1154.720117	16.271091
31.004262	1158.008555	16.276109
30.776315	1150.699192	16.281127
30.828094	1146.818308	16.286144
30.856700	1152.337954	16.291162
31.440654	1150.121325	16.296179
31.320042	1155.247936	16.301197
30.821711	1156.065114	16.306215
30.815666	1149.203261	16.311232
31.116874	1139.563336	16.316250
30.692352	1153.421123	16.321267
30.748772	1165.767686	16.326285
31.079964	1174.358258	16.331303
31.307091	1180.248932	16.336320
31.190115	1190.885051	16.341338
31.406700	1180.918835	16.346355
31.778942	1177.507485	16.351373
31.558037	1181.563185	16.356391
31.707067	1178.464273	16.361408
31.891432	1173.245671	16.366426
31.641540	1179.597793	16.371443
31.843796	1166.859173	16.376461
31.718154	1175.933143	16.381479
31.578878	1162.816430	16.386496
31.639163	1153.392662	16.391514
31.821054	1166.614228	16.396531
31.768802	1151.410490	16.401549
31.684915	1151.087244	16.406567
31.871756	1147.013368	16.411584
31.622623	1146.093586	16.416602
31.680952	1166.567306	16.421619
32.038131	1171.288977	16.426637
31.849522	1175.380422	16.431655
32.058062	1175.156825	16.436672
31.905104	1179.097874	16.441690
31.945520	1177.743392	16.446707
32.057864	1169.017569	16.451725
32.180621	1176.345267	16.456743
31.829205	1177.370241	16.461760
32.078842	1168.745215	16.466778
31.994971	1170.844321	16.471795
32.535338	1163.668815	16.476813
32.180170	1166.704626	16.481831
32.123063	1162.531230	16.486848
32.276890	1169.303434	16.491866
32.262804	1170.952556	16.496883
32.047794	1164.850727	16.501901
31.991385	1163.293047	16.506919
32.437747	1171.229777	16.511936
32.436327	1153.686806	16.516954
32.117694	1165.026717	16.521971
31.993025	1168.953813	16.526989
31.809939	1173.245715	16.532007
32.079408	1165.177501	16.537024
32.437066	1163.055160	16.542042
32.254850	1170.925399	16.547059
32.539055	1173.587124	16.552077
32.808518	1191.239927	16.557095
32.684581	1183.037822	16.562112
32.874086	1166.360975	16.567130
32.267182	1167.624885	16.572147
32.383244	1175.304420	16.577165
32.559835	1185.538228	16.582183
32.693884	1195.344692	16.587200
32.972678	1192.739440	16.592218
32.843593	1189.889364	16.597235
33.034287	1187.326476	16.602253
33.096758	1200.301288	16.607271
33.337289	1188.336734	16.612288
33.321617	1183.818537	16.617306
32.736139	1170.980606	16.622323
33.088789	1158.084308	16.627341
32.790055	1162.531497	16.632359
32.710329	1163.247312	16.637376
33.265910	1185.667728	16.642394
33.022677	1195.392792	16.647411
32.792136	1183.438876	16.652429
32.965711	1189.674708	16.657447
32.789764	1190.493955	16.662464
32.811654	1186.603670	16.667482
32.626114	1195.836635	16.672499
33.669900	1206.981327	16.677517
33.438359	1203.886475	16.682535
33.394908	1181.469276	16.687552
33.598008	1177.249660	16.692570
33.291848	1189.274983	16.697587
33.547850	1172.233608	16.702605
33.574457	1173.438959	16.707623
33.561680	1184.122946	16.712640
33.676494	1174.105328	16.717658
33.347852	1178.568302	16.722675
33.391025	1177.933795	16.727693
33.622202	1194.834542	16.732711
33.843926	1200.350149	16.737728
33.803036	1203.434943	16.742746
33.537035	1193.787916	16.747763
34.082530	1202.114677	16.752781
34.010178	1187.982146	16.757799
33.832438	1181.721789	16.762816
33.803241	1176.884868	16.767834
33.644402	1179.938133	16.772851
33.697607	1186.141252	16.777869
33.852238	1200.268502	16.782887
33.956779	1205.816955	16.787904
34.471921	1197.698534	16.792922
34.146226	1202.590463	16.797939
34.005117	1176.331946	16.802957
34.071664	1194.150815	16.807975
33.703469	1202.225329	16.812992
34.263011	1184.372647	16.818010
34.106689	1206.873595	16.823027
34.368841	1205.002422	16.828045
34.320353	1193.889312	16.833063
33.936136	1198.081168	16.838080
34.471335	1188.956004	16.843098
34.084780	1210.156658	16.848115
34.158813	1198.268983	16.853133
34.528084	1190.801440	16.858151
34.219254	1198.298646	16.863168
34.779518	1184.252414	16.868186
34.634240	1198.587932	16.873203
34.534610	1208.647167	16.878221
34.499907	1206.028990	16.883239
34.482494	1196.803194	16.888256
34.922171	1201.415769	16.893274
34.413923	1200.096876	16.898291
34.367383	1190.929209	16.903309
34.592234	1201.502958	16.908327
34.225449	1202.542968	16.913344
34.631716	1201.458888	16.918362
34.499409	1207.159939	16.923379
34.686045	1193.608993	16.928397
34.700138	1202.756646	16.933415
34.541366	1209.380529	16.938432
34.925937	1213.012502	16.943450
34.907589	1224.790617	16.948467
34.887779	1215.524294	16.953485
35.304153	1216.267957	16.958503
35.163984	1221.638373	16.963520
35.325719	1210.313980	16.968538
35.061710	1216.009298	16.973555
35.209073	1220.338174	16.978573
35.415390	1221.042980	16.983591
35.188994	1221.167159	16.988608
35.499860	1222.618179	16.993626
35.234904	1229.746623	16.998643
35.558462	1218.089689	17.003661
35.412271	1216.669012	17.008679
35.177001	1216.771012	17.013696
35.508453	1213.965458	17.018714
35.333689	1222.781460	17.023731
35.517939	1220.194428	17.028749
35.653125	1225.833952	17.033767
35.429001	1211.497523	17.038784
35.598285	1210.772120	17.043802
35.569558	1227.258194	17.048819
35.481550	1217.257162	17.053837
35.631745	1217.297689	17.058855
35.335097	1223.473250	17.063872
35.290024	1214.530269	17.068890
35.633263	1215.903769	17.073907
35.286864	1205.638797	17.078925
35.263806	1217.208452	17.083943
35.223730	1231.302293	17.088960
35.800944	1234.430088	17.093978
36.081772	1249.564407	17.098995
35.834689	1256.545301	17.104013
35.938498	1244.841595	17.109031
35.838124	1251.129007	17.114048
36.234160	1245.964709	17.119066
36.187508	1255.329714	17.124083
36.099241	1243.272837	17.129101
36.119369	1245.725015	17.134119
36.106934	1249.769510	17.139136
36.565952	1238.551835	17.144154
36.413013	1238.782273	17.149171
36.320755	1243.791139	17.154189
36.630493	1243.283999	17.159207
36.481044	1252.918644	17.164224
36.513744	1242.443757	17.169242
36.497956	1249.118784	17.174259
36.178464	1240.932103	17.179277
36.506466	1240.909670	17.184295
36.482877	1248.386580	17.189312
36.804772	1242.927378	17.194330
36.245948	1252.117667	17.199347
36.502394	1244.207210	17.204365
36.593856	1246.314544	17.209383
36.317787	1256.809347	17.214400
36.310882	1250.026232	17.219418
36.218187	1258.144928	17.224435
36.507637	1250.424252	17.229453
36.414685	1254.034866	17.234471
36.346114	1268.452599	17.239488
36.884252	1275.701520	17.244506
36.783302	1275.514695	17.249523
36.604227	1283.515051	17.254541
36.886454	1280.616665	17.259559
36.997092	1286.725727	17.264576
36.853553	1277.611226	17.269594
36.986682	1281.473645	17.274611
37.029432	1276.584320	17.279629
37.219045	1269.546495	17.284647
36.977051	1270.038090	17.289664
37.252652	1271.059027	17.294682
37.290009	1284.137017	17.299699
37.112823	1274.581159	17.304717
37.180228	1264.168360	17.309735
37.291760	1271.370486	17.314752
37.424877	1299.738209	17.319770
37.520553	1311.377091	17.324787
37.716032	1291.779710	17.329805
38.103208	1275.563554	17.334823
37.900255	1279.338002	17.339840
37.381096	1277.394799	17.344858
37.677971	1276.790613	17.349875
37.456476	1270.707076	17.354893
37.802406	1259.441356	17.359911
37.893748	1271.526047	17.364928
37.873492	1269.054987	17.369946
37.931832	1266.256800	17.374963
37.908962	1266.521548	17.379981
37.710004	1259.345928	17.384999
37.544494	1284.742722	17.390016
37.660891	1272.332297	17.395034
37.954635	1267.904724	17.400051
37.711596	1271.201089	17.405069
37.747109	1272.379859	17.410087
37.829382	1273.719481	17.415104
37.803260	1275.239977	17.420122
38.041259	1298.957008	17.425139
38.326091	1301.911230	17.430157
38.419490	1291.291352	17.435175
38.261430	1300.502699	17.440192
38.099677	1298.169026	17.445210
38.368528	1294.730095	17.450227
38.154644	1299.151210	17.455245
37.976139	1287.918767	17.460263
38.007762	1296.217426	17.465280
38.155994	1295.563014	17.470298
38.050174	1291.733964	17.475315
38.145461	1288.047444	17.480333
38.555818	1291.804310	17.485351
38.234715	1300.742794	17.490368
38.379150	1309.514236	17.495386
38.689176	1324.492973	17.500403
38.527566	1321.942202	17.505421
38.789764	1323.688849	17.510439
38.848532	1326.362960	17.515456
38.711074	1320.273865	17.520474
39.000682	1315.994797	17.525491
38.831751	1309.844661	17.530509
39.098511	1312.024719	17.535527
39.160744	1324.140837	17.540544
39.046847	1306.838980	17.545562
39.174167	1299.918037	17.550579
38.844517	1294.867877	17.555597
38.911527	1286.279771	17.560615
38.634446	1295.853003	17.565632
39.026769	1303.672587	17.570650
38.915139	1307.423042	17.575667
38.950657	1319.614200	17.580685
38.937140	1320.399685	17.585703
39.072463	1320.941218	17.590720
39.226474	1321.327192	17.595738
39.470157	1316.847815	17.600755
39.319215	1323.841722	17.605773
39.591969	1310.821183	17.610791
39.368945	1315.618127	17.615808
39.107639	1312.307782	17.620826
39.282231	1312.117912	17.625843
39.232061	1317.016275	17.630861
39.609100	1330.858082	17.635879
39.581958	1342.492981	17.640896
39.626172	1337.836202	17.645914
39.659448	1333.835527	17.650931
39.624724	1344.715035	17.655949
39.773285	1343.565082	17.660967
39.914229	1339.264098	17.665984
39.807827	1335.090648	17.671002
39.988871	1331.248874	17.676019
39.705504	1339.324092	17.681037
39.816395	1337.706680	17.686055
39.973978	1343.701318	17.691072
40.273546	1334.129165	17.696090
40.235770	1336.165889	17.701107
40.227387	1332.845091	17.706125
39.945830	1335.729201	17.711143
40.228454	1333.464650	17.716160
40.215629	1333.202425	17.721178
40.031437	1336.704917	17.726195
40.109373	1343.393355	17.731213
39.982097	1330.446030	17.736231
40.098954	1341.826737	17.741248
40.315830	1332.667308	17.746266
40.376910	1339.185404	17.751283
40.301654	1341.690562	17.756301
40.558619	1333.006070	17.761319
40.229209	1328.811558	17.766336
40.418737	1335.378380	17.771354
40.910552	1352.848063	17.776371
40.919400	1358.924626	17.781389
41.017451	1347.380627	17.786407
40.752740	1336.979841	17.791424
40.610131	1332.571501	17.796442
40.956812	1327.526727	17.801459
40.549612	1331.006581	17.806477
40.855302	1331.750600	17.811495
41.047286	1345.615642	17.816512
41.071119	1355.922695	17.821530
41.276087	1342.769796	17.826547
40.914937	1340.140735	17.831565
40.909739	1323.423973	17.836583
41.038589	1336.224732	17.841600
41.044237	1356.944643	17.846618
41.296098	1353.546159	17.851635
40.940968	1352.814720	17.856653
41.409810	1348.776039	17.861671
41.368121	1359.189495	17.866688
41.317815	1364.293956	17.871706
41.628182	1357.954110	17.876723
41.346321	1364.965769	17.881741
41.448998	1356.208343	17.886759
41.256637	1350.047770	17.891776
41.197167	1360.465635	17.896794
41.295092	1357.683139	17.901811
41.124822	1365.800109	17.906829
41.451809	1350.194347	17.911847
41.281824	1357.878698	17.916864
41.362338	1369.233763	17.921882
41.989519	1361.585008	17.926899
41.899485	1365.667078	17.931917
41.878538	1364.242143	17.936935
41.855569	1346.291827	17.941952
41.616629	1359.281816	17.946970
42.201444	1357.058731	17.951987
41.999460	1378.944329	17.957005
41.995416	1369.049347	17.962023
42.043731	1364.300673	17.967040
41.878439	1375.893138	17.972058
42.133044	1383.032392	17.977075
41.758835	1381.820302	17.982093
42.250175	1373.082681	17.987111
42.539555	1378.954072	17.992128
42.281131	1384.734292	17.997146
42.454731	1371.362219	18.002163
42.199881	1391.317569	18.007181
42.385698	1366.780107	18.012199
42.592174	1377.056476	18.017216
42.485283	1376.069949	18.022234
42.544484	1373.192955	18.027251
42.502724	1381.264272	18.032269
42.414772	1380.966837	18.037287
42.667137	1376.808518	18.042304
42.323837	1381.409167	18.047322
42.646057	1373.030414	18.052339
42.525788	1383.743488	18.057357
42.732395	1380.353002	18.062375
42.534847	1378.375798	18.067392
42.532422	1379.494563	18.072410
42.650585	1386.452664	18.077427
42.790928	1398.984239	18.082445
43.089489	1399.518619	18.087463
43.578292	1400.754098	18.092480
43.163317	1390.290722	18.097498
43.454003	1385.618217	18.102515
43.182413	1384.407851	18.107533
43.446596	1379.487110	18.112551
43.318841	1374.606067	18.117568
43.077893	1368.596374	18.122586
43.218960	1366.563600	18.127603
43.041409	1368.569138	18.132621
43.220273	1379.054399	18.137639
43.578704	1386.826739	18.142656
43.138684	1394.720909	18.147674
43.477449	1395.558755	18.152691
43.311518	1399.544402	18.157709
43.253886	1393.709952	18.162727
43.637896	1389.661194	18.167744
43.358786	1391.273956	18.172762
43.463570	1385.448215	18.177779
43.864844	1394.420990	18.182797
44.023950	1387.096971	18.187815
43.892284	1388.140395	18.192832
43.883789	1394.782867	18.197850
43.907280	1393.366572	18.202867
43.635122	1395.464277	18.207885
43.576173	1401.419539	18.212903
43.762138	1399.923852	18.217920
43.705073	1421.390012	18.222938
44.032513	1427.145244	18.227955
44.151991	1429.664978	18.232973
44.057847	1432.624610	18.237991
44.427121	1431.316759	18.243008
44.590031	1421.903192	18.248026
44.319263	1420.667524	18.253043
44.319833	1419.698463	18.258061
44.305445	1424.251392	18.263079
44.720834	1416.740201	18.268096
44.096276	1426.304439	18.273114
44.380993	1414.760505	18.278131
44.200213	1419.206263	18.283149
44.198474	1418.062970	18.288167
44.471410	1413.350816	18.293184
44.707035	1427.216841	18.298202
45.035906	1436.929481	18.303219
44.754137	1431.547602	18.308237
45.040670	1427.050347	18.313255
44.824242	1414.494680	18.318272
44.677375	1418.979074	18.323290
44.892501	1417.378063	18.328307
44.850993	1432.412972	18.333325
44.798639	1446.740209	18.338343
45.150070	1439.413808	18.343360
45.064527	1437.911079	18.348378
45.146504	1433.584866	18.353395
45.454496	1451.672281	18.358413
44.858445	1442.524448	18.363431
45.170277	1436.426574	18.368448
45.135640	1437.377451	18.373466
45.125601	1432.892884	18.378483
45.169093	1439.127547	18.383501
45.097002	1438.056818	18.388519
45.353147	1429.405433	18.393536
45.124697	1442.409553	18.398554
45.225530	1456.039131	18.403571
45.367035	1463.140621	18.408589
45.472056	1459.405316	18.413607
45.868672	1455.856313	18.418624
45.713240	1463.521096	18.423642
46.135505	1460.292037	18.428659
46.234678	1466.642099	18.433677
46.154527	1465.541193	18.438695
45.938216	1460.150437	18.443712
45.843751	1459.921677	18.448730
46.126965	1461.680720	18.453747
46.209500	1465.080934	18.458765
45.918189	1468.031117	18.463783
45.959436	1460.526087	18.468800
45.819009	1467.494792	18.473818
46.536935	1460.740704	18.478835
46.621671	1460.805829	18.483853
46.311598	1466.470838	18.488871
46.483483	1469.172553	18.493888
46.576368	1461.788273	18.498906
46.488006	1444.966659	18.503923
45.980653	1442.224044	18.508941
46.097313	1456.360747	18.513959
46.475838	1459.411744	18.518976
46.336091	1467.797603	18.523994
46.296659	1458.872447	18.529011
46.471217	1459.972431	18.534029
46.212201	1461.740868	18.539047
46.523249	1464.181296	18.544064
46.550483	1480.358294	18.549082
46.526128	1485.320236	18.554099
46.567812	1491.844640	18.559117
46.419980	1485.544776	18.564135
46.703234	1482.348892	18.569152
46.785422	1481.376249	18.574170
46.918543	1477.921169	18.579187
47.396736	1484.234391	18.584205
47.104347	1504.731486	18.589223
47.265124	1482.636749	18.594240
47.283224	1478.369472	18.599258
47.299594	1481.621369	18.604275
47.426001	1483.441600	18.609293
47.074301	1497.077317	18.614311
47.408560	1505.982199	18.619328
47.468979	1517.180140	18.624346
47.759980	1510.819721	18.629363
47.929970	1510.275087	18.634381
47.619594	1500.476056	18.639399
47.747322	1479.481397	18.644416
47.742493	1476.896158	18.649434
47.725925	1483.527374	18.654451
47.664189	1476.560992	18.659469
47.966515	1495.896748	18.664487
48.217816	1494.591976	18.669504
47.659192	1480.141883	18.674522
48.154278	1485.351318	18.679539
47.940458	1487.200637	18.684557
47.852652	1487.900453	18.689575
47.956646	1495.520737	18.694592
47.712078	1502.329890	18.699610
48.174064	1501.369037	18.704627
48.141595	1503.931892	18.709645
48.115091	1496.233159	18.714663
48.368270	1499.428420	18.719680
48.373382	1501.373386	18.724698
48.547130	1497.583067	18.729715
48.515923	1492.110872	18.734733
48.653701	1493.845922	18.739751
48.385203	1498.955339	18.744768
48.468831	1499.476809	18.749786
48.797605	1494.658199	18.754803
48.770767	1494.811902	18.759821
48.400231	1495.350743	18.764839
48.711790	1492.128321	18.769856
48.137261	1490.753901	18.774874
48.468029	1492.709854	18.779891
48.934900	1502.718277	18.784909
48.567223	1525.862173	18.789927
49.173245	1509.920738	18.794944
49.247574	1515.961757	18.799962
49.124706	1519.583499	18.804979
49.279114	1521.834989	18.809997
49.213466	1524.467631	18.815015
49.668353	1517.130985	18.820032
49.481347	1497.940380	18.825050
48.879034	1489.682255	18.830067
49.333842	1495.930000	18.835085
49.217679	1505.310970	18.840103
49.301695	1517.489843	18.845120
49.329580	1519.210961	18.850138
49.425963	1522.446961	18.855155
49.900874	1517.831551	18.860173
49.414006	1523.210176	18.865191
49.717403	1522.562470	18.870208
49.847133	1515.678792	18.875226
49.408053	1520.892496	18.880243
49.663919	1515.124406	18.885261
49.688106	1522.449123	18.890279
49.699367	1507.730375	18.895296
49.285180	1519.306017	18.900314
49.823697	1533.410128	18.905331
50.008769	1539.403611	18.910349
49.699649	1544.835694	18.915367
50.049680	1534.752003	18.920384
50.032049	1541.768799	18.925402
49.942060	1535.978777	18.930419
50.424898	1535.270996	18.935437
50.361015	1547.473479	18.940455
50.276241	1538.679771	18.945472
50.482530	1539.463249	18.950490
50.276748	1542.596432	18.955507
50.569757	1529.529996	18.960525
50.003592	1537.508851	18.965543
50.329465	1541.990253	18.970560
51.007962	1553.385381	18.975578
50.818926	1559.306398	18.980595
51.337078	1557.748284	18.985613
50.917141	1546.193923	18.990631
50.926212	1536.016742	18.995648
50.620487	1542.425114	19.000666
50.751814	1529.448954	19.005683
50.850916	1537.137679	19.010701
50.792393	1554.687506	19.015719
50.901698	1555.488023	19.020736
50.771683	1555.242908	19.025754
50.739599	1559.669716	19.030771
50.912644	1558.174500	19.035789
50.546122	1566.093220	19.040807
51.068638	1566.491222	19.045824
51.209681	1587.771881	19.050842
51.632947	1583.053004	19.055859
51.688954	1583.797529	19.060877
51.602764	1585.717742	19.065895
51.524940	1595.778486	19.070912
51.911437	1581.875987	19.075930
51.665671	1579.469149	19.080947
51.784573	1576.749333	19.085965
51.825901	1580.143561	19.090983
51.778706	1585.426926	19.096000
51.941250	1571.682845	19.101018
52.031470	1585.484122	19.106035
51.968743	1573.893224	19.111053
51.582175	1582.793556	19.116071
51.833770	1588.400503	19.121088
52.012935	1582.532935	19.126106
51.763837	1588.847354	19.131123
52.131908	1574.702412	19.136141
52.170040	1590.286346	19.141159
52.366069	1582.132089	19.146176
51.955807	1574.279010	19.151194
52.345608	1584.759097	19.156211
52.243589	1577.602465	19.161229
52.644031	1578.084428	19.166247
52.552503	1580.744802	19.171264
52.686517	1584.515928	19.176282
52.384660	1578.934278	19.181299
52.602473	1584.302796	19.186317
52.847653	1602.081097	19.191335
52.765708	1602.466956	19.196352
53.031334	1595.388538	19.201370
52.749318	1603.823904	19.206387
53.274183	1593.330052	19.211405
53.133257	1609.614234	19.216423
52.928836	1597.210647	19.221440
53.031096	1598.893173	19.226458
52.939913	1601.029685	19.231475
52.938602	1598.012861	19.236493
53.219488	1597.200432	19.241511
53.271223	1605.643923	19.246528
53.156659	1593.005790	19.251546
52.836385	1605.530775	19.256563
53.133419	1597.395008	19.261581
52.916093	1600.869813	19.266599
53.400761	1620.672156	19.271616
53.559374	1638.599585	19.276634
53.316376	1623.422621	19.281651
53.480236	1635.849980	19.286669
53.663150	1629.203156	19.291687
53.703206	1633.300734	19.296704
54.058793	1630.733498	19.301722
53.684964	1641.137202	19.306739
54.191889	1627.220175	19.311757
53.768752	1636.417377	19.316775
53.753908	1624.518358	19.321792
54.019265	1626.423414	19.326810
53.683729	1632.682424	19.331827
54.119299	1628.924251	19.336845
53.953581	1637.465358	19.341863
54.235713	1647.014136	19.346880
54.280735	1658.282281	19.351898
54.114446	1666.464850	19.356915
54.591279	1649.165907	19.361933
54.184938	1661.075461	19.366951
54.147992	1664.296576	19.371968
54.534223	1648.360153	19.376986
54.612243	1646.365709	19.382003
54.619498	1652.409616	19.387021
54.966234	1648.561786	19.392039
54.630584	1656.216084	19.397056
54.853269	1648.085853	19.402074
54.832990	1650.542970	19.407091
55.028423	1646.970949	19.412109
54.864701	1647.588498	19.417127
55.068309	1653.670307	19.422144
55.110128	1645.303081	19.427162
54.889714	1654.677177	19.432179
55.150581	1670.733761	19.437197
55.246338	1684.721439	19.442215
55.280464	1675.765542	19.447232
55.521567	1676.464826	19.452250
55.495833	1682.289066	19.457267
55.765624	1679.928984	19.462285
55.855770	1664.459753	19.467303
55.796445	1673.425931	19.472320
55.648867	1649.582159	19.477338
55.751583	1661.596151	19.482355
55.652996	1652.909967	19.487373
55.669667	1664.278591	19.492391
55.720136	1663.620878	19.497408
56.025415	1671.163539	19.502426
55.956590	1674.932429	19.507443
55.573966	1675.389833	19.512461
56.082046	1663.407393	19.517479
55.844299	1683.123677	19.522496
56.141243	1670.235812	19.527514
55.796260	1674.882436	19.532531
55.822555	1677.791451	19.537549
55.582685	1681.134592	19.542567
56.084274	1690.006613	19.547584
56.190444	1696.788240	19.552602
55.660213	1707.835127	19.557619
56.239319	1702.114518	19.562637
56.440293	1695.047935	19.567655
56.424566	1704.076392	19.572672
56.907344	1720.640335	19.577690
56.738349	1735.365554	19.582707
56.932076	1722.138600	19.587725
57.024176	1708.606969	19.592743
56.733565	1703.113139	19.597760
56.997897	1709.029560	19.602778
56.892448	1722.981720	19.607795
57.200541	1720.143619	19.612813
57.511265	1726.790394	19.617831
57.199109	1712.305482	19.622848
56.972276	1693.441862	19.627866
57.030596	1712.725586	19.632883
57.121580	1720.477050	19.637901
57.256726	1718.868313	19.642919
57.242872	1733.630139	19.647936
57.591677	1725.434135	19.652954
57.431585	1727.894685	19.657971
57.182852	1728.742870	19.662989
58.005506	1720.139399	19.668007
57.526563	1735.505500	19.673024
57.538780	1723.010629	19.678042
57.542079	1728.927785	19.683059
57.248065	1724.913127	19.688077
57.582446	1728.776608	19.693095
57.563301	1744.209394	19.698112
57.955442	1736.476807	19.703130
57.814282	1745.761245	19.708147
57.914401	1735.998839	19.713165
58.107771	1747.804965	19.718183
58.474561	1741.750111	19.723200
58.498456	1742.174151	19.728218
58.269750	1742.062746	19.733235
58.134703	1729.839891	19.738253
58.194481	1737.119716	19.743271
58.543469	1765.384717	19.748288
58.718363	1759.879554	19.753306
58.616843	1754.407460	19.758323
58.760453	1760.793037	19.763341
58.866762	1761.244834	19.768359
58.949824	1756.512513	19.773376
58.983231	1768.238771	19.778394
58.733651	1753.223169	19.783411
59.217772	1767.764048	19.788429
59.115319	1760.033241	19.793447
58.806271	1759.200047	19.798464
59.337843	1754.501597	19.803482
59.533928	1749.951028	19.808499
59.594901	1761.543898	19.813517
59.503472	1759.150171	19.818535
59.389963	1757.148501	19.823552
59.728499	1754.723962	19.828570
59.239185	1746.611261	19.833587
59.333569	1745.540702	19.838605
59.608650	1760.891981	19.843623
59.401402	1758.878517	19.848640
59.704258	1765.208815	19.853658
59.417887	1764.301218	19.858675
59.511983	1762.442620	19.863693
59.777851	1756.243406	19.868711
59.484921	1756.702239	19.873728
59.500424	1762.494767	19.878746
59.472348	1776.764975	19.883763
59.635493	1781.715995	19.888781
59.868123	1780.571479	19.893799
59.869551	1796.669575	19.898816
59.985101	1774.550145	19.903834
60.211250	1796.696861	19.908851
59.954293	1796.527040	19.913869
60.297128	1798.613246	19.918887
60.385008	1820.866991	19.923904
60.716326	1825.710984	19.928922
60.899105	1815.609727	19.933939
60.627759	1815.198381	19.938957
60.930135	1822.260238	19.943975
60.877700	1831.804289	19.948992
60.752412	1815.810827	19.954010
60.964008	1809.804289	19.959027
60.663443	1825.500688	19.964045
60.984872	1809.816669	19.969063
60.912017	1806.218180	19.974080
60.869689	1812.693205	19.979098
60.784202	1798.845316	19.984115
60.919242	1805.973175	19.989133
61.167064	1806.304879	19.994151
61.137779	1823.630144	19.999168
61.634908	1828.274664	20.004186
61.886064	1823.556415	20.009203
61.432328	1826.422457	20.014221
61.934233	1825.055673	20.019239
61.417547	1816.769545	20.024256
61.333704	1821.245584	20.029274
61.747951	1829.017917	20.034291
61.898350	1822.671920	20.039309
61.889871	1815.821151	20.044327
61.686604	1822.463417	20.049344
61.803189	1828.165920	20.054362
62.016813	1823.986913	20.059379
61.973611	1829.337370	20.064397
62.192716	1827.875682	20.069415
61.740130	1826.549419	20.074432
61.957381	1834.018114	20.079450
61.975746	1848.944806	20.084467
62.213464	1847.443968	20.089485
62.364523	1846.222792	20.094503
62.218952	1859.734741	20.099520
62.580535	1850.566069	20.104538
62.456326	1864.773042	20.109555
62.646689	1857.879534	20.114573
62.782276	1849.487799	20.119591
62.624264	1854.908484	20.124608
63.085869	1843.586116	20.129626
62.837553	1852.357599	20.134643
62.813352	1852.183694	20.139661
62.912972	1840.735008	20.144679
62.921370	1856.069139	20.149696
63.068717	1865.370568	20.154714
63.311217	1873.771211	20.159731
63.458207	1875.043941	20.164749
63.866475	1862.495232	20.169767
63.242981	1859.286559	20.174784
63.791065	1861.434427	20.179802
63.792489	1846.924543	20.184819
63.782997	1842.833019	20.189837
63.697361	1832.881518	20.194855
63.547073	1838.842087	20.199872
63.813448	1836.786121	20.204890
63.708694	1837.433599	20.209907
63.674429	1859.854747	20.214925
64.139612	1860.260331	20.219943
63.994414	1871.978975	20.224960
64.155971	1864.651180	20.229978
63.995468	1865.272943	20.234995
64.085943	1875.028616	20.240013
64.308745	1865.520268	20.245031
64.333433	1867.193173	20.250048
64.153781	1868.664282	20.255066
64.294836	1867.908744	20.260083
64.275393	1866.647114	20.265101
64.292342	1859.229124	20.270119
64.190623	1866.298812	20.275136
64.262186	1885.115035	20.280154
64.539539	1890.919342	20.285171
64.513223	1901.296129	20.290189
64.759052	1894.862524	20.295207
64.579356	1896.398136	20.300224
64.767481	1894.123403	20.305242
65.273261	1893.028131	20.310259
64.758477	1898.982353	20.315277
65.242112	1915.521216	20.320295
65.502539	1921.257448	20.325312
65.470291	1914.905929	20.330330
65.573989	1911.976116	20.335347
65.023746	1925.121643	20.340365
65.095731	1913.911689	20.345383
65.091977	1919.493417	20.350400
65.254265	1920.854947	20.355418
65.395838	1911.969861	20.360435
65.576089	1930.200945	20.365453
65.788389	1935.383281	20.370471
65.672191	1942.346775	20.375488
65.768037	1947.640496	20.380506
66.528408	1935.523221	20.385523
66.263304	1931.758726	20.390541
66.588112	1926.894991	20.395559
66.172979	1912.884052	20.400576
66.098789	1906.403944	20.405594
66.216199	1905.965210	20.410611
66.323850	1927.660684	20.415629
66.218916	1935.924856	20.420647
66.336431	1942.674902	20.425664
66.531362	1934.990962	20.430682
66.425458	1931.252991	20.435699
66.474606	1927.705802	20.440717
66.601465	1936.217732	20.445735
66.654024	1926.277164	20.450752
66.556604	1928.052919	20.455770
66.728417	1919.885032	20.460787
66.487777	1932.935578	20.465805
67.034975	1935.222027	20.470823
67.204214	1946.873287	20.475840
67.101521	1956.639368	20.480858
67.144930	1958.114242	20.485875
66.739002	1963.214272	20.490893
67.139633	1945.109149	20.495911
67.118052	1963.007513	20.500928
66.934699	1962.731569	20.505946
67.845376	1964.129495	20.510963
67.970967	1973.340081	20.515981
68.059149	1979.226500	20.520999
67.831911	1964.619252	20.526016
68.044050	1956.583342	20.531034
68.136553	1944.901325	20.536051
67.960421	1956.949016	20.541069
67.883774	1941.944967	20.546087
67.807738	1954.181190	20.551104
68.190231	1963.563164	20.556122
68.557456	1976.485357	20.561139
68.089266	1984.072870	20.566157
68.206725	1990.911037	20.571175
68.648305	1986.692487	20.576192
68.489561	1985.863626	20.581210
68.546557	1982.672254	20.586227
68.099086	1983.358658	20.591245
68.398481	1985.168672	20.596263
68.678966	1981.340759	20.601280
68.709435	1977.930246	20.606298
69.080966	1974.534561	20.611315
68.836574	1983.465947	20.616333
68.885719	1977.475807	20.621351
68.742681	1999.384399	20.626368
69.163053	1996.687219	20.631386
69.476579	1995.459001	20.636403
69.227098	2003.527607	20.641421
69.201922	2002.380139	20.646439
69.450530	2005.217590	20.651456
69.439672	2009.317101	20.656474
69.541346	1998.437407	20.661491
69.406713	2001.488554	20.666509
69.822795	2001.620398	20.671527
69.832525	2006.364721	20.676544
69.604470	2004.011616	20.681562
70.011950	1989.013690	20.686579
69.550884	1995.596469	20.691597
69.596209	1997.841834	20.696615
70.092071	1994.657556	20.701632
69.970416	2001.310485	20.706650
70.079825	2000.753472	20.711667
70.192271	2024.987228	20.716685
70.330438	2023.717755	20.721703
70.511046	2024.274119	20.726720
70.110414	2025.009685	20.731738
70.136531	2023.295604	20.736755
70.248628	2032.137139	20.741773
70.317725	2025.305361	20.746791
70.517733	2020.960153	20.751808
70.422337	2025.788888	20.756826
70.964133	2036.285968	20.761843
70.946944	2043.855078	20.766861
71.078672	2044.996547	20.771879
71.209425	2048.840677	20.776896
71.231294	2048.664143	20.781914
71.454114	2039.146241	20.786931
71.365048	2045.405449	20.791949
71.361440	2045.866918	20.796967
71.472027	2038.628963	20.801984
71.410182	2040.381755	20.807002
71.562360	2047.277335	20.812019
71.375985	2044.223860	20.817037
71.509953	2041.971898	20.822055
71.670922	2041.670935	20.827072
71.645140	2047.564543	20.832090
71.762963	2040.385209	20.837107
71.437608	2038.497506	20.842125
71.700096	2068.071515	20.847143
72.382642	2067.382208	20.852160
72.003250	2072.665238	20.857178
72.393228	2064.600910	20.862195
72.409768	2066.375813	20.867213
72.794485	2061.387648	20.872231
72.791861	2066.481606	20.877248
72.590773	2066.123543	20.882266
72.808733	2061.523771	20.887283
72.644066	2068.438425	20.892301
72.528941	2068.867339	20.897319
72.789667	2066.826399	20.902336
72.791176	2071.781271	20.907354
72.816256	2067.964175	20.912371
72.631113	2070.389450	20.917389
72.910934	2061.458631	20.922407
73.029225	2063.368322	20.927424
72.820308	2071.197685	20.932442
72.884340	2063.471629	20.937459
72.920828	2084.006760	20.942477
73.192283	2077.957534	20.947495
73.224417	2087.946027	20.952512
73.227727	2093.846027	20.957530
73.547220	2084.816058	20.962547
73.543912	2083.599029	20.967565
73.230149	2089.857906	20.972583
73.524526	2090.715462	20.977600
73.653111	2108.870064	20.982618
73.793125	2110.932030	20.987635
73.925114	2108.008677	20.992653
73.960234	2112.248754	20.997671
73.852769	2109.642015	21.002688
73.659466	2117.080367	21.007706
74.137998	2116.909666	21.012723
74.398299	2132.661681	21.017741
74.480275	2128.363578	21.022759
74.656152	2137.322425	21.027776
74.706725	2140.191481	21.032794
74.860649	2123.629325	21.037811
75.002975	2131.987891	21.042829
74.973197	2141.486060	21.047847
75.144710	2131.339189	21.052864
75.178999	2141.736372	21.057882
74.940422	2123.470254	21.062899
74.879042	2136.762964	21.067917
75.130041	2124.973730	21.072935
75.168269	2130.627499	21.077952
75.188417	2135.508632	21.082970
75.278570	2112.700590	21.087987
75.060702	2125.513291	21.093005
74.943288	2128.182611	21.098023
75.731942	2134.526845	21.103040
75.816073	2161.255501	21.108058
75.729871	2152.148607	21.113075
76.015220	2161.794746	21.118093
75.814754	2158.037187	21.123111
76.048608	2156.307268	21.128128
75.651435	2160.347298	21.133146
76.081658	2146.432572	21.138163
76.082620	2153.441980	21.143181
75.739488	2153.979615	21.148199
76.120215	2153.826083	21.153216
76.060523	2165.784592	21.158234
76.388022	2182.598777	21.163251
76.672255	2171.895915	21.168269
76.491219	2169.313482	21.173287
76.991223	2167.242239	21.178304
76.691084	2171.216461	21.183322
76.758547	2165.641758	21.188339
77.171184	2171.029768	21.193357
76.904917	2165.321086	21.198375
77.126537	2162.534444	21.203392
77.110846	2159.260241	21.208410
77.334060	2163.857313	21.213427
77.024493	2164.970057	21.218445
77.156047	2179.857018	21.223463
77.344785	2165.659876	21.228480
76.988095	2172.038894	21.233498
77.627422	2191.562525	21.238515
77.912599	2197.801450	21.243533
77.693217	2196.982244	21.248551
78.202058	2196.224675	21.253568
77.731210	2207.786298	21.258586
78.243029	2189.044927	21.263603
78.172322	2188.299545	21.268621
77.902756	2197.382943	21.273639
78.279905	2187.964607	21.278656
77.727808	2198.939840	21.283674
78.108695	2187.530977	21.288691
77.978729	2196.968078	21.293709
77.879102	2197.177441	21.298727
78.059196	2199.752141	21.303744
78.351523	2214.755078	21.308762
78.427110	2227.489613	21.313779
78.167436	2233.831952	21.318797
78.209289	2227.871187	21.323815
78.816142	2239.046262	21.328832
78.945500	2245.016676	21.333850
78.943655	2245.256066	21.338867
79.242192	2238.606260	21.343885
79.264174	2246.833066	21.348903
79.727482	2235.470014	21.353920
79.587354	2240.707085	21.358938
79.617396	2233.047709	21.363955
79.595083	2241.030670	21.368973
79.456733	2232.551045	21.373991
79.970662	2237.566628	21.379008
79.612604	2233.761031	21.384026
79.498801	2239.525603	21.389043
79.788838	2229.835619	21.394061
79.664270	2259.259373	21.399079
79.930443	2255.110405	21.404096
80.049305	2262.288261	21.409114
80.189877	2267.189564	21.414131
80.211213	2265.373966	21.419149
80.071384	2260.359262	21.424167
80.801080	2258.104300	21.429184
80.687368	2264.955076	21.434202
80.618211	2255.735283	21.439219
80.990048	2255.601259	21.444237
80.563298	2264.018396	21.449255
80.677803	2260.652620	21.454272
80.588620	2269.527969	21.459290
80.997662	2279.157609	21.464307
81.193695	2291.881647	21.469325
80.933812	2307.104085	21.474343
81.207239	2289.519060	21.479360
80.960544	2298.230773	21.484378
81.213157	2290.137100	21.489395
81.444542	2278.690655	21.494413
81.167215	2284.827398	21.499431
81.179183	2288.633115	21.504448
81.340020	2311.819828	21.509466
81.534087	2310.377031	21.514483
81.710162	2311.701794	21.519501
81.783124	2316.171072	21.524519
82.098671	2305.802904	21.529536
82.187017	2312.680474	21.534554
82.002719	2315.028573	21.539571
82.063493	2308.570810	21.544589
81.910790	2308.362332	21.549607
82.057661	2328.217940	21.554624
82.355642	2339.566620	21.559642
82.281959	2332.305204	21.564659
82.441852	2342.227881	21.569677
82.562436	2346.801264	21.574695
82.860281	2331.413827	21.579712
82.847434	2331.177542	21.584730
82.730704	2331.575258	21.589747
83.142920	2338.855818	21.594765
82.824905	2363.769136	21.599783
82.973617	2361.241057	21.604800
83.118892	2370.044473	21.609818
83.280022	2359.723700	21.614835
83.525835	2361.940299	21.619853
83.532074	2365.853134	21.624871
83.669362	2358.590313	21.629888
83.772615	2362.479811	21.634906
83.322790	2364.204055	21.639923
83.918916	2368.399584	21.644941
83.877677	2387.910087	21.649959
84.091284	2383.812726	21.654976
84.215558	2387.695733	21.659994
83.912509	2380.131079	21.665011
84.636301	2370.934217	21.670029
84.183389	2385.904361	21.675047
84.170576	2377.042823	21.680064
84.454156	2374.702458	21.685082
84.820602	2365.607412	21.690099
85.100941	2373.078126	21.695117
84.564026	2375.703480	21.700135
84.699183	2364.321864	21.705152
84.623003	2362.065609	21.710170
85.193957	2367.667559	21.715187
85.032484	2358.696024	21.720205
84.646999	2370.705077	21.725223
85.393665	2391.766862	21.730240
85.411526	2390.319120	21.735258
85.429218	2406.272934	21.740275
85.530472	2400.945235	21.745293
85.565886	2398.621627	21.750311
85.885120	2401.052264	21.755328
85.824396	2393.747850	21.760346
85.651315	2406.036895	21.765363
86.033807	2386.106973	21.770381
85.827385	2408.496642	21.775399
85.853874	2395.199787	21.780416
86.037083	2402.870842	21.785434
85.331763	2391.205568	21.790451
86.102457	2406.486371	21.795469
86.394877	2425.050992	21.800487
86.177960	2430.272846	21.805504
86.280754	2431.186929	21.810522
86.549863	2422.609973	21.815539
86.737183	2408.131237	21.820557
86.336920	2420.477756	21.825575
86.520157	2418.310694	21.830592
86.939921	2411.722494	21.835610
86.853581	2438.330185	21.840627
87.074045	2434.872752	21.845645
87.381688	2432.825856	21.850663
86.970099	2436.610270	21.855680
87.097362	2443.318095	21.860698
87.166023	2442.059671	21.865715
87.717052	2419.079341	21.870733
87.488711	2444.055578	21.875751
87.439978	2452.875823	21.880768
87.694945	2463.278949	21.885786
87.521656	2466.082301	21.890803
87.961145	2465.132063	21.895821
87.801087	2462.584772	21.900839
88.447616	2455.356325	21.905856
88.098560	2468.494639	21.910874
88.176316	2457.130756	21.915891
88.454323	2452.223973	21.920909
88.533045	2467.567200	21.925927
88.511935	2482.299482	21.930944
89.077525	2492.380166	21.935962
88.646671	2488.603411	21.940979
88.746993	2490.815700	21.945997
88.646225	2485.392762	21.951015
88.728728	2490.107549	21.956032
88.829916	2482.435910	21.961050
88.508511	2497.767462	21.966067
89.019842	2490.852366	21.971085
88.956578	2514.338631	21.976103
89.302878	2508.843611	21.981120
89.576651	2506.680976	21.986138
89.549886	2516.507688	21.991155
89.503221	2512.395160	21.996173
89.654700	2515.484167	22.001191
89.746799	2506.885834	22.006208
89.704348	2517.209002	22.011226
90.048329	2534.825612	22.016243
90.340566	2527.961952	22.021261
89.981723	2535.099705	22.026279
90.413341	2542.413458	22.031296
90.478606	2530.380579	22.036314
90.246305	2535.630094	22.041331
90.229712	2530.045845	22.046349
90.275920	2532.189687	22.051367
90.241351	2533.020282	22.056384
90.450759	2551.222329	22.061402
90.499453	2542.250990	22.066419
90.992047	2545.364267	22.071437
91.192452	2551.489442	22.076455
90.914013	2559.279024	22.081472
91.365080	2550.601404	22.086490
91.101797	2558.697685	22.091507
91.002770	2546.959205	22.096525
91.384140	2561.822455	22.101543
91.740609	2575.223554	22.106560
91.794342	2576.991016	22.111578
91.848969	2574.953769	22.116595
92.137607	2579.671898	22.121613
91.894756	2580.080291	22.126631
91.849455	2576.348220	22.131648
92.116129	2592.300292	22.136666
91.715270	2584.703146	22.141683
92.051244	2572.815841	22.146701
92.307780	2588.207139	22.151719
92.305569	2598.799242	22.156736
92.781434	2601.549450	22.161754
92.662856	2605.958118	22.166771
93.051555	2603.600957	22.171789
93.042771	2588.634184	22.176807
92.888918	2595.047111	22.181824
93.313942	2602.568811	22.186842
93.324088	2595.663578	22.191859
93.251645	2596.309868	22.196877
93.144041	2593.890264	22.201895
93.006936	2605.548428	22.206912
93.271559	2595.214920	22.211930
93.125646	2598.172029	22.216947
93.532607	2609.789851	22.221965
93.526515	2625.039010	22.226983
93.521995	2639.130120	22.232000
93.662121	2623.908319	22.237018
93.526420	2626.089832	22.242035
93.861824	2639.569859	22.247053
94.009336	2648.678273	22.252071
94.313527	2650.661440	22.257088
94.784847	2640.711817	22.262106
94.424529	2659.864552	22.267123
94.511549	2649.168405	22.272141
94.912162	2647.139691	22.277159
94.706446	2641.493528	22.282176
94.737057	2651.348937	22.287194
94.586091	2663.184760	22.292211
94.783386	2659.330610	22.297229
95.039390	2677.985524	22.302247
94.937436	2680.474715	22.307264
95.470918	2665.758047	22.312282
95.254106	2687.944508	22.317299
95.071255	2686.848084	22.322317
95.327258	2668.759622	22.327335
95.147897	2678.296937	22.332352
95.638915	2696.074354	22.337370
95.680718	2703.671369	22.342387
95.671578	2703.940247	22.347405
96.052632	2707.056400	22.352423
96.194341	2706.587813	22.357440
96.478219	2694.036993	22.362458
96.015790	2709.890718	22.367475
96.082587	2705.339233	22.372493
96.446292	2701.673270	22.377511
96.369160	2713.095427	22.382528
96.396324	2713.477287	22.387546
96.931416	2730.625548	22.392563
96.937777	2722.106831	22.397581
97.088165	2724.412640	22.402599
97.254986	2732.441223	22.407616
97.323872	2712.477487	22.412634
97.026278	2721.099246	22.417651
96.906142	2726.638489	22.422669
97.081060	2722.398542	22.427687
97.297522	2728.706075	22.432704
97.386112	2741.354825	22.437722
97.512988	2748.664574	22.442739
97.817944	2750.726290	22.447757
97.715648	2751.282173	22.452775
97.847710	2749.510213	22.457792
97.999750	2745.639659	22.462810
98.195408	2751.624095	22.467827
98.388467	2765.221323	22.472845
98.385803	2763.027220	22.477863
98.552119	2774.272958	22.482880
98.661180	2770.606680	22.487898
98.596207	2775.853982	22.492915
98.938792	2771.125573	22.497933
98.895530	2770.425338	22.502951
98.833976	2774.166608	22.507968
98.832184	2760.852691	22.512986
99.088785	2774.940839	22.518003
99.057298	2773.548121	22.523021
99.393042	2786.535054	22.528039
99.173172	2796.198463	22.533056
99.619281	2799.976779	22.538074
99.424756	2812.883893	22.543091
99.633989	2800.753113	22.548109
99.541197	2800.379333	22.553127
99.622360	2805.910893	22.558144
99.885642	2800.079767	22.563162
99.885321	2820.057838	22.568179
99.924240	2825.902117	22.573197
100.443076	2826.058495	22.578215
100.237142	2830.526780	22.583232
100.399863	2826.400441	22.588250
100.443479	2823.903986	22.593267
100.478494	2818.515905	22.598285
100.404473	2827.672340	22.603303
100.751018	2845.122954	22.608320
100.956639	2838.468816	22.613338
100.898767	2855.003073	22.618355
100.920389	2847.859133	22.623373
101.205318	2849.655050	22.628391
101.257277	2850.441190	22.633408
101.024687	2851.200336	22.638426
101.147505	2862.213961	22.643443
101.560498	2864.732770	22.648461
101.694785	2859.595493	22.653479
101.550834	2864.463708	22.658496
102.167177	2868.778870	22.663514
101.740957	2870.162752	22.668531
102.182722	2862.162884	22.673549
102.443814	2865.781941	22.678567
102.500879	2884.555364	22.683584
102.914874	2890.463355	22.688602
102.226261	2882.738100	22.693619
102.589245	2887.538865	22.698637
103.065298	2897.413086	22.703655
102.652771	2893.968379	22.708672
103.138986	2900.693906	22.713690
103.089091	2881.867383	22.718707
103.224884	2889.149825	22.723725
103.550564	2884.330474	22.728743
103.496544	2876.653486	22.733760
103.754147	2876.989169	22.738778
103.561136	2882.693472	22.743795
103.705872	2878.875176	22.748813
103.899914	2875.071830	22.753831
103.663349	2880.621043	22.758848
103.621426	2874.214801	22.763866
103.847679	2893.876828	22.768883
103.808663	2905.114506	22.773901
104.340827	2909.598058	22.778919
103.936769	2904.339734	22.783936
104.210140	2906.508764	22.788954
104.122123	2914.819560	22.793971
104.338807	2929.382233	22.798989
104.794848	2930.388688	22.804007
104.591270	2931.277716	22.809024
104.961481	2928.814118	22.814042
105.033424	2931.171797	22.819059
105.137491	2939.978198	22.824077
105.514544	2949.198865	22.829095
105.466461	2957.025079	22.834112
105.762770	2946.492774	22.839130
105.698395	2952.054675	22.844147
105.668277	2960.832929	22.849165
106.059652	2958.155150	22.854183
105.898391	2961.071518	22.859200
105.981422	2950.304994	22.864218
106.096813	2954.205302	22.869235
105.967714	2952.488330	22.874253
106.204615	2953.573776	22.879271
106.097744	2948.801348	22.884288
106.274084	2942.427134	22.889306
106.524038	2949.459364	22.894323
106.829086	2967.339133	22.899341
107.230834	2962.423464	22.904359
107.020306	2981.186977	22.909376
107.555160	2968.140478	22.914394
107.270254	2942.802316	22.919411
106.903489	2956.972729	22.924429
107.341838	2954.174981	22.929447
107.408142	2971.203992	22.934464
107.379379	2962.004053	22.939482
107.470344	2973.516812	22.944499
107.415374	2961.153509	22.949517
107.555460	2959.488005	22.954535
107.572886	2985.650680	22.959552
107.581418	2984.868237	22.964570
107.750505	2988.260517	22.969587
107.891680	2991.069674	22.974605
107.969943	3012.028140	22.979623
108.294992	3019.208106	22.984640
108.621684	3014.099877	22.989658
108.406471	3028.933665	22.994675
108.284604	3023.605133	22.999693
109.032661	3035.422191	23.004711
108.946288	3055.936595	23.009728
109.153785	3047.683732	23.014746
109.266739	3049.156281	23.019763
109.434151	3053.864792	23.024781
109.450952	3036.877473	23.029799
109.783941	3036.931343	23.034816
109.901965	3046.648016	23.039834
109.662423	3035.866789	23.044851
109.657520	3041.964341	23.049869
110.436233	3026.945495	23.054887
110.116313	3038.724396	23.059904
109.965856	3039.962067	23.064922
110.400391	3044.183566	23.069939
110.191649	3057.782994	23.074957
110.828199	3059.718734	23.079975
110.500204	3066.581241	23.084992
110.880317	3057.714846	23.090010
111.079720	3060.504507	23.095027
111.158069	3060.510882	23.100045
111.181624	3054.115358	23.105063
111.156525	3062.639594	23.110080
110.941294	3064.018168	23.115098
111.021319	3063.936178	23.120115
111.044963	3073.330474	23.125133
111.108026	3073.223658	23.130151
111.145634	3083.510078	23.135168
111.549246	3072.115784	23.140186
112.028629	3096.594083	23.145203
111.630027	3108.757639	23.150221
112.259050	3101.284687	23.155239
112.439579	3115.525307	23.160256
112.005032	3118.448309	23.165274
112.333760	3106.593979	23.170291
111.971491	3107.806434	23.175309
112.014782	3118.057362	23.180327
111.951087	3129.934708	23.185344
112.210066	3138.010176	23.190362
112.736067	3144.533616	23.195379
112.848955	3170.611395	23.200397
113.237505	3166.121734	23.205415
113.360361	3168.522462	23.210432
113.364050	3173.850991	23.215450
113.713300	3171.334063	23.220467
113.721388	3171.223426	23.225485
114.116969	3159.760340	23.230503
113.754610	3167.225391	23.235520
113.942732	3157.715443	23.240538
114.122109	3149.204286	23.245555
114.116148	3166.705200	23.250573
114.178222	3164.423629	23.255591
114.590014	3172.500709	23.260608
114.753926	3164.147754	23.265626
115.079532	3166.833936	23.270643
114.911089	3170.814168	23.275661
115.004534	3173.678167	23.280679
114.984432	3164.828323	23.285696
114.999257	3155.736155	23.290714
115.329828	3164.376004	23.295731
115.031445	3175.356341	23.300749
115.036389	3162.859034	23.305767
115.424737	3179.510507	23.310784
115.471271	3198.325343	23.315802
115.740045	3192.796023	23.320819
115.755071	3193.199496	23.325837
115.605787	3180.399543	23.330855
115.680277	3203.409520	23.335872
115.936428	3212.106099	23.340890
116.405929	3225.856330	23.345907
116.052926	3220.362424	23.350925
116.446522	3226.616761	23.355943
116.589370	3230.582773	23.360960
116.606261	3244.085044	23.365978
117.208215	3244.585293	23.370995
117.112785	3254.315687	23.376013
117.023691	3247.094026	23.381031
116.841497	3255.980871	23.386048
117.003463	3249.354746	23.391066
117.899008	3250.941663	23.396083
117.571796	3272.517340	23.401101
117.933555	3269.439921	23.406119
118.211999	3272.541884	23.411136
118.080469	3274.490783	23.416154
118.222226	3270.311028	23.421171
118.158374	3271.394896	23.426189
118.520019	3270.943141	23.431207
118.439586	3268.974528	23.436224
118.205879	3265.252654	23.441242
118.466252	3262.660997	23.446259
118.340733	3261.626179	23.451277
118.527286	3267.978046	23.456295
118.892840	3259.154755	23.461312
118.936079	3279.289335	23.466330
118.916207	3283.566052	23.471347
118.969101	3289.072414	23.476365
119.307342	3286.106504	23.481383
119.193623	3291.693707	23.486400
119.484687	3303.856013	23.491418
119.740743	3312.708413	23.496435
119.476838	3316.760540	23.501453
119.706819	3309.992969	23.506471
120.154705	3317.313178	23.511488
119.990796	3326.664387	23.516506
120.451396	3331.872928	23.521523
120.480175	3339.615512	23.526541
120.328399	3341.608550	23.531559
120.651859	3342.668427	23.536576
120.708119	3346.750534	23.541594
120.904840	3341.376595	23.546611
120.834920	3339.403936	23.551629
120.965191	3361.207282	23.556647
121.246013	3355.815995	23.561664
121.365687	3363.050117	23.566682
121.475679	3369.025656	23.571699
121.325257	3368.965462	23.576717
121.661200	3380.517356	23.581735
121.885618	3380.959816	23.586752
121.657251	3388.738706	23.591770
122.034516	3384.236621	23.596787
121.735989	3394.185913	23.601805
121.653262	3398.139954	23.606823
122.416039	3411.050710	23.611840
122.498517	3414.612646	23.616858
122.929367	3425.708162	23.621875
122.582708	3419.148897	23.626893
123.227377	3412.551928	23.631911
123.137104	3419.362537	23.636928
123.119494	3433.687762	23.641946
123.616454	3432.826635	23.646963
123.636650	3437.648416	23.651981
123.582819	3434.572724	23.656999
124.068920	3437.915352	23.662016
123.912152	3435.215548	23.667034
124.092287	3430.477435	23.672051
124.170720	3442.619484	23.677069
124.107820	3426.331909	23.682087
123.971596	3430.481699	23.687104
124.121989	3436.504313	23.692122
124.432433	3432.796323	23.697139
124.553034	3452.106248	23.702157
124.469036	3445.732420	23.707175
125.124672	3450.710898	23.712192
124.701826	3460.343390	23.717210
124.606638	3453.771546	23.722227
124.680661	3457.896475	23.727245
125.021060	3478.636832	23.732263
125.550522	3476.320810	23.737280
125.445284	3484.976847	23.742298
125.516347	3482.560071	23.747315
125.858723	3484.380736	23.752333
125.829220	3514.275624	23.757351
126.046564	3499.718655	23.762368
125.983463	3515.587453	23.767386
126.149160	3513.126479	23.772403
126.153046	3513.257998	23.777421
126.375293	3530.477541	23.782439
126.896982	3528.921826	23.787456
126.836183	3547.427783	23.792474
127.217015	3532.642557	23.797491
127.072828	3542.727809	23.802509
127.123962	3531.302834	23.807527
127.560977	3529.405073	23.812544
127.408007	3536.870750	23.817562
127.460564	3535.541646	23.822579
127.858014	3537.237119	23.827597
127.631335	3552.243958	23.832615
128.033976	3542.398289	23.837632
127.920307	3547.898267	23.842650
127.956208	3541.176479	23.847667
128.261933	3551.984478	23.852685
128.161529	3558.213104	23.857703
128.446853	3571.753114	23.862720
128.204806	3572.064647	23.867738
128.704657	3576.655038	23.872755
128.635473	3580.909813	23.877773
129.019880	3590.120279	23.882791
129.118208	3590.501829	23.887808
129.308716	3606.811696	23.892826
129.193545	3596.208449	23.897843
129.376012	3608.775337	23.902861
129.506877	3621.116840	23.907879
130.041901	3618.979258	23.912896
130.221579	3621.071303	23.917914
130.345526	3621.842862	23.922931
130.511982	3617.015623	23.927949
130.413906	3624.614969	23.932967
130.803133	3611.827891	23.937984
130.594364	3619.295427	23.943002
130.937674	3612.370418	23.948019
130.974105	3620.775831	23.953037
130.924900	3632.739376	23.958055
131.433633	3632.463175	23.963072
131.252730	3645.488415	23.968090
131.394141	3635.729169	23.973107
131.514623	3631.950730	23.978125
131.701720	3638.733737	23.983143
131.908149	3629.701971	23.988160
131.545911	3641.810612	23.993178
131.348556	3631.981095	23.998195
132.006310	3644.830933	24.003213
131.922771	3659.807194	24.008231
132.055187	3664.902206	24.013248
132.330788	3671.133859	24.018266
132.211519	3680.212301	24.023283
132.289950	3685.016227	24.028301
132.380319	3695.009124	24.033319
132.973356	3693.205247	24.038336
132.721997	3711.287916	24.043354
133.287995	3724.724323	24.048371
133.738846	3719.047786	24.053389
133.511815	3721.096137	24.058407
133.708330	3730.766142	24.063424
133.454596	3731.616801	24.068442
133.864324	3735.564787	24.073459
133.810192	3742.740280	24.078477
133.642333	3761.726895	24.083495
134.107925	3753.320000	24.088512
134.183315	3760.282917	24.093530
134.356446	3775.979822	24.098547
134.681917	3775.271092	24.103565
134.878520	3781.133878	24.108583
135.176425	3778.086989	24.113600
135.074536	3769.403210	24.118618
135.182632	3781.947494	24.123635
135.290073	3794.257480	24.128653
135.475014	3795.739868	24.133671
135.944619	3798.415012	24.138688
135.815552	3796.604326	24.143706
136.064232	3784.828289	24.148723
136.018309	3793.040050	24.153741
136.040552	3800.890901	24.158759
136.169609	3814.757328	24.163776
136.077720	3816.651207	24.168794
136.300210	3820.052474	24.173811
136.534624	3832.343823	24.178829
136.630300	3847.778622	24.183847
136.913772	3843.325965	24.188864
137.026137	3851.853917	24.193882
137.342034	3855.860161	24.198899
137.379863	3852.348136	24.203917
137.282256	3867.805906	24.208935
137.850853	3873.659765	24.213952
137.997411	3883.068024	24.218970
138.064392	3868.467799	24.223987
138.187456	3864.463127	24.229005
137.771289	3874.938085	24.234023
138.437121	3871.922979	24.239040
138.518899	3893.715974	24.244058
138.841318	3890.295439	24.249075
139.028690	3893.002227	24.254093
138.721482	3895.217563	24.259111
139.060287	3896.376512	24.264128
138.978396	3901.497908	24.269146
139.218233	3898.227412	24.274163
139.129926	3897.142563	24.279181
139.203409	3918.026002	24.284199
139.701868	3922.339048	24.289216
139.687185	3921.200768	24.294234
139.663157	3928.093873	24.299251
139.728284	3931.007375	24.304269
140.057956	3931.305639	24.309287
140.243786	3944.927937	24.314304
140.010423	3941.850081	24.319322
140.118092	3939.119036	24.324339
140.723876	3956.038800	24.329357
140.428446	3961.231233	24.334375
140.818747	3966.466160	24.339392
141.303088	3971.350992	24.344410
141.535045	3975.125224	24.349427
141.676128	3979.357604	24.354445
141.870963	3976.888762	24.359463
141.800636	3980.415415	24.364480
142.168981	3982.164355	24.369498
142.239766	3985.084832	24.374515
142.313812	3981.837603	24.379533
142.110983	3977.826648	24.384551
142.707309	3973.556129	24.389568
142.556420	3980.292493	24.394586
142.249479	4004.146454	24.399603
142.654136	4008.467401	24.404621
142.797003	4016.124505	24.409639
142.866382	4012.597972	24.414656
143.079481	4027.795557	24.419674
143.408330	4036.706019	24.424691
143.640950	4027.228533	24.429709
143.381754	4036.326356	24.434727
143.839440	4043.626495	24.439744
143.670498	4060.560554	24.444762
143.946891	4064.404815	24.449779
144.277639	4059.414364	24.454797
144.009682	4078.107412	24.459815
144.445588	4071.850228	24.464832
144.825822	4091.132191	24.469850
144.643271	4089.473948	24.474867
144.817218	4091.703852	24.479885
144.637851	4108.501180	24.484903
145.167382	4116.007013	24.489920
145.233833	4125.495064	24.494938
145.356100	4132.511256	24.499955
145.604024	4125.582337	24.504973
145.587585	4143.031811	24.509991
146.186180	4150.053094	24.515008
146.199211	4152.258317	24.520026
146.411526	4152.723973	24.525043
146.749335	4148.072196	24.530061
146.474875	4153.329003	24.535079
146.773889	4138.839405	24.540096
146.992202	4146.146294	24.545114
146.777113	4141.094163	24.550131
146.877206	4151.075597	24.555149
146.923308	4159.539562	24.560167
147.157216	4173.851372	24.565184
147.429344	4167.015331	24.570202
147.454146	4182.020478	24.575219
147.641522	4192.091860	24.580237
147.812955	4198.138182	24.585255
147.873196	4202.333171	24.590272
147.866888	4197.081754	24.595290
148.293846	4224.006542	24.600307
148.538724	4225.378729	24.605325
148.757195	4232.451216	24.610343
148.992735	4227.142351	24.615360
149.088202	4229.431200	24.620378
149.137588	4235.370345	24.625395
149.534101	4231.233875	24.630413
149.535978	4255.241963	24.635431
149.632036	4252.961099	24.640448
149.732785	4248.472161	24.645466
149.594342	4248.592552	24.650483
150.044667	4252.376095	24.655501
149.950366	4260.360623	24.660519
150.169942	4270.665280	24.665536
150.172768	4276.080879	24.670554
149.953595	4289.460487	24.675571
150.498193	4291.326111	24.680589
150.881734	4303.174798	24.685607
151.107639	4307.567600	24.690624
151.536726	4290.847421	24.695642
151.392562	4295.956069	24.700659
151.881080	4312.953944	24.705677
152.002192	4322.954957	24.710695
152.501546	4314.959288	24.715712
152.114561	4321.588703	24.720730
152.210059	4325.059109	24.725747
152.362100	4323.735314	24.730765
152.470409	4329.851540	24.735783
152.191729	4318.203992	24.740800
152.608754	4312.411481	24.745818
152.648085	4336.039285	24.750835
152.871303	4329.803315	24.755853
153.033309	4348.917455	24.760871
153.102845	4347.612318	24.765888
153.376294	4351.048067	24.770906
153.095040	4369.029326	24.775923
153.445779	4380.349169	24.780941
153.618139	4380.099844	24.785959
154.094339	4396.168384	24.790976
154.165550	4393.550839	24.795994
154.439643	4398.464617	24.801011
154.864438	4401.742518	24.806029
154.434323	4401.410672	24.811047
154.758910	4397.217184	24.816064
154.812169	4392.390433	24.821082
154.807265	4419.322287	24.826099
155.083803	4431.562585	24.831117
155.647381	4421.858233	24.836135
155.687827	4424.191284	24.841152
155.698261	4430.334168	24.846170
155.568696	4429.247203	24.851187
155.811205	4442.806650	24.856205
156.187836	4451.670417	24.861223
155.876744	4448.679577	24.866240
156.196866	4448.804741	24.871258
156.245548	4476.647757	24.876275
156.023666	4476.962383	24.881293
156.471829	4485.281412	24.886311
156.575163	4495.266497	24.891328
156.777171	4507.698100	24.896346
156.754878	4518.085544	24.901363
157.142332	4527.710691	24.906381
157.692643	4549.151487	24.911399
157.816976	4532.222382	24.916416
157.995538	4549.545280	24.921434
158.038535	4565.171740	24.926451
158.520042	4569.547472	24.931469
158.627257	4572.429219	24.936487
158.566168	4561.944874	24.941504
158.701089	4555.934498	24.946522
158.707896	4582.278720	24.951539
159.097864	4585.651896	24.956557
159.395823	4594.861837	24.961575
159.631578	4596.607607	24.966592
159.686333	4593.194187	24.971610
159.535077	4595.555467	24.976627
160.193537	4595.301802	24.981645
160.261037	4616.695377	24.986663
160.001717	4622.253588	24.991680
160.216194	4608.448819	24.996698
160.417702	4628.998983	25.001715
160.769574	4637.406611	25.006733
160.809631	4646.460247	25.011751
160.767904	4643.401250	25.016768
161.175306	4639.978012	25.021786
160.908215	4659.758832	25.026803
161.354747	4670.576683	25.031821
161.701533	4668.311637	25.036839
161.620321	4668.706893	25.041856
162.114466	4683.367115	25.046874
161.910374	4699.602657	25.051891
162.090828	4694.459742	25.056909
162.421825	4703.868233	25.061927
162.325294	4704.188839	25.066944
162.484314	4702.111842	25.071962
162.409795	4718.100188	25.076979
162.928145	4727.953188	25.081997
163.121575	4715.407200	25.087015
163.198926	4725.553132	25.092032
163.528597	4743.100756	25.097050
163.714482	4760.370028	25.102067
163.334160	4753.176743	25.107085
163.713309	4757.033915	25.112103
164.068022	4759.925803	25.117120
164.657359	4759.047526	25.122138
164.308467	4780.209571	25.127155
164.638506	4765.341530	25.132173
164.655260	4769.261985	25.137191
164.486669	4784.398486	25.142208
165.004612	4794.881723	25.147226
165.000133	4797.885162	25.152243
165.262194	4801.456569	25.157261
165.409759	4810.613529	25.162279
165.411823	4833.115262	25.167296
166.068031	4821.614061	25.172314
165.947298	4836.541597	25.177331
165.957169	4839.862148	25.182349
166.432678	4854.597887	25.187367
166.372535	4856.154859	25.192384
166.489706	4856.216409	25.197402
166.460613	4875.680306	25.202419
166.984918	4874.083927	25.207437
167.143379	4876.538264	25.212455
167.265375	4902.380102	25.217472
167.742033	4900.675675	25.222490
167.741314	4905.335284	25.227507
168.073902	4905.001407	25.232525
168.028980	4906.780161	25.237543
168.175250	4915.452798	25.242560
168.201474	4924.634681	25.247578
168.517686	4936.859638	25.252595
168.693646	4933.637647	25.257613
168.705219	4941.733109	25.262631
168.948878	4960.943592	25.267648
169.188138	4963.534533	25.272666
169.583441	4949.069698	25.277683
169.662084	4960.939995	25.282701
170.260308	4967.469276	25.287719
170.159529	4975.444211	25.292736
170.253764	4968.593681	25.297754
170.575243	4981.425156	25.302771
170.588708	4981.751046	25.307789
170.996921	4983.273487	25.312807
171.071135	4977.346566	25.317824
171.135230	4965.916048	25.322842
171.075169	4975.924362	25.327859
171.151712	4994.655694	25.332877
171.462542	4996.661738	25.337895
171.332069	4998.152055	25.342912
171.691917	4994.522340	25.347930
171.639363	5007.862664	25.352947
171.673754	5024.280817	25.357965
172.070264	5026.380983	25.362983
172.112338	5038.512059	25.368000
172.425005	5040.190555	25.373018
172.684961	5050.652170	25.378035
172.738851	5073.068126	25.383053
172.991925	5068.221100	25.388071
172.762520	5072.535675	25.393088
173.063754	5078.057402	25.398106
173.349244	5090.277159	25.403123
173.458959	5090.616028	25.408141
173.728734	5102.135786	25.413159
173.889695	5117.972956	25.418176
174.429631	5119.702553	25.423194
174.371658	5126.545776	25.428211
174.519661	5141.183758	25.433229
174.842183	5141.421048	25.438247
174.984239	5145.459299	25.443264
175.172120	5146.249857	25.448282
175.334970	5151.876276	25.453299
175.282927	5173.019882	25.458317
175.530972	5168.445035	25.463335
175.504815	5172.429081	25.468352
175.772831	5191.522699	25.473370
175.947884	5204.398167	25.478387
176.048524	5200.105632	25.483405
176.249208	5209.688630	25.488423
176.660950	5223.049536	25.493440
176.493541	5216.763755	25.498458
176.866153	5234.260281	25.503475
176.687152	5247.989154	25.508493
177.626760	5236.147445	25.513511
177.287533	5257.322793	25.518528
177.620795	5254.778966	25.523546
178.058664	5281.261836	25.528563
177.922410	5278.020314	25.533581
178.098581	5269.595770	25.538599
178.223690	5291.963731	25.543616
178.559277	5290.804120	25.548634
178.759709	5303.226423	25.553651
178.932106	5312.778596	25.558669
179.555282	5314.659370	25.563687
179.370744	5322.064898	25.568704
179.748147	5328.639773	25.573722
180.182153	5321.766384	25.578739
179.987645	5323.439228	25.583757
180.046712	5325.761587	25.588775
180.095027	5345.600036	25.593792
180.669471	5339.207741	25.598810
180.741872	5348.291269	25.603827
180.580628	5344.912109	25.608845
180.811803	5352.432323	25.613863
181.038278	5384.233371	25.618880
181.174801	5377.056509	25.623898
181.427828	5374.755170	25.628915
181.303409	5385.442721	25.633933
181.293165	5389.827082	25.638951
181.247864	5409.332030	25.643968
181.696055	5416.518732	25.648986
182.086521	5430.276573	25.654003
181.987619	5441.521019	25.659021
182.379872	5437.864792	25.664039
182.746270	5459.901101	25.669056
183.009805	5463.746213	25.674074
182.994579	5463.421357	25.679092
183.537314	5475.676739	25.684109
183.606990	5488.892593	25.689127
183.704421	5495.599501	25.694144
183.587132	5496.705423	25.699162
184.053689	5496.915039	25.704180
184.180199	5522.073594	25.709197
184.662628	5517.846766	25.714215
184.498379	5521.465856	25.719232
184.772067	5507.481665	25.724250
185.148055	5535.834649	25.729268
185.127597	5545.889746	25.734285
185.550126	5542.950084	25.739303
185.801436	5548.168410	25.744320
185.835296	5547.012825	25.749338
186.283575	5565.122335	25.754356
186.209963	5572.363189	25.759373
186.426040	5572.132053	25.764391
186.428934	5577.446634	25.769408
186.850298	5561.571974	25.774426
186.934761	5578.125158	25.779444
187.309417	5592.572475	25.784461
187.474762	5585.861373	25.789479
187.743953	5593.408693	25.794496
187.747364	5596.714710	25.799514
188.110111	5604.695551	25.804532
188.035591	5616.990446	25.809549
188.153866	5605.602720	25.814567
188.301913	5616.523141	25.819584
188.036515	5627.528360	25.824602
188.479500	5637.736216	25.829620
188.601442	5646.535106	25.834637
188.844447	5642.281113	25.839655
189.182006	5672.495571	25.844672
189.246352	5672.954975	25.849690
189.732661	5676.362616	25.854708
189.791501	5699.873067	25.859725
190.248090	5693.154826	25.864743
190.223365	5691.287144	25.869760
190.194138	5697.466776	25.874778
190.674221	5711.538659	25.879796
190.802220	5719.743437	25.884813
191.164369	5723.740470	25.889831
191.275747	5724.034247	25.894848
191.362902	5713.224920	25.899866
191.855046	5728.641768	25.904884
191.635310	5748.900331	25.909901
191.951066	5742.292631	25.914919
192.099920	5747.093876	25.919936
191.939385	5743.845106	25.924954
192.419807	5754.961252	25.929972
192.370252	5763.746640	25.934989
192.736448	5767.747761	25.940007
192.873296	5774.805686	25.945024
192.856292	5791.882724	25.950042
193.390374	5797.700393	25.955060
193.074276	5813.187954	25.960077
193.685554	5819.717903	25.965095
193.716713	5833.689959	25.970112
193.927162	5840.779454	25.975130
194.157144	5841.563341	25.980148
194.518590	5865.027391	25.985165
194.858760	5854.535590	25.990183
194.838936	5864.853572	25.995200
195.342333	5879.176014	26.000218
195.520755	5875.956576	26.005236
195.818550	5886.770720	26.010253
196.064531	5884.158095	26.015271
196.057048	5879.454617	26.020288
196.493895	5879.391263	26.025306
196.696791	5893.028387	26.030324
196.660475	5919.753214	26.035341
196.820757	5901.117462	26.040359
197.023788	5914.551608	26.045376
197.109600	5904.555839	26.050394
197.452553	5910.697473	26.055412
197.340956	5932.580176	26.060429
197.379588	5926.650680	26.065447
197.613947	5933.070043	26.070464
197.812584	5953.163065	26.075482
198.063688	5962.405729	26.080500
197.913163	5966.043982	26.085517
198.244182	5990.269922	26.090535
198.638895	5993.992775	26.095552
198.884466	6016.525158	26.100570
199.103412	6016.882829	26.105588
199.179151	6022.151341	26.110605
199.384371	6037.177611	26.115623
199.680233	6043.579352	26.120640
199.621131	6047.214065	26.125658
200.079727	6057.119978	26.130676
200.319370	6071.478360	26.135693
200.716196	6074.460572	26.140711
200.949217	6079.239068	26.145728
201.246183	6091.329593	26.150746
201.583920	6085.776408	26.155764
201.940279	6088.786316	26.160781
201.866730	6091.017433	26.165799
202.171678	6088.564523	26.170816
201.956341	6086.197697	26.175834
202.398878	6087.351315	26.180852
202.362494	6100.692409	26.185869
202.378416	6104.657411	26.190887
202.365296	6114.623610	26.195904
202.690281	6124.719232	26.200922
202.871529	6129.492623	26.205940
202.952592	6145.085583	26.210957
202.985989	6171.608573	26.215975
203.773902	6179.046759	26.220992
203.592635	6181.444542	26.226010
203.953281	6182.869276	26.231028
204.094940	6209.626836	26.236045
204.251111	6203.362219	26.241063
204.549553	6219.358039	26.246080
204.518826	6235.160881	26.251098
205.058972	6249.027019	26.256116
205.116920	6254.288223	26.261133
205.321191	6260.959567	26.266151
205.511576	6261.701798	26.271168
205.923664	6286.942017	26.276186
206.085778	6287.613228	26.281204
206.222509	6297.322784	26.286221
206.699368	6297.983949	26.291239
206.938565	6309.359261	26.296256
206.991761	6312.013936	26.301274
207.259452	6320.671983	26.306292
207.497095	6328.273490	26.311309
207.759815	6332.204720	26.316327
208.372092	6326.294555	26.321344
208.549131	6332.553292	26.326362
208.726964	6337.608167	26.331380
208.759762	6341.749136	26.336397
209.418148	6357.927691	26.341415
209.380459	6353.630123	26.346432
209.202290	6370.935717	26.351450
209.404171	6359.172963	26.356468
209.492732	6351.153576	26.361485
209.400454	6369.495799	26.366503
209.744576	6380.045653	26.371520
209.636524	6390.413469	26.376538
210.165726	6408.634644	26.381556
210.063254	6430.162586	26.386573
210.462908	6435.035798	26.391591
210.678968	6437.344324	26.396608
210.738169	6465.229546	26.401626
211.076682	6458.539227	26.406644
211.065043	6471.163903	26.411661
211.482868	6477.932694	26.416679
211.907844	6486.129900	26.421696
212.033905	6492.399978	26.426714
212.441943	6518.906358	26.431732
212.518247	6523.331546	26.436749
212.937585	6518.008306	26.441767
213.055618	6521.732128	26.446784
213.061747	6545.441938	26.451802
213.546446	6552.650922	26.456820
213.891864	6552.673741	26.461837
213.615734	6554.117406	26.466855
214.055038	6556.551652	26.471872
214.105840	6568.968979	26.476890
214.534029	6583.343439	26.481908
214.591601	6583.051800	26.486925
215.026706	6600.436141	26.491943
215.330216	6601.435729	26.496960
215.278094	6607.970290	26.501978
215.865898	6603.639035	26.506996
215.868591	6600.679550	26.512013
215.822863	6622.044518	26.517031
216.371095	6622.505498	26.522048
216.249190	6634.239955	26.527066
216.588680	6635.897846	26.532084
216.542017	6659.905000	26.537101
216.733568	6663.809899	26.542119
216.948322	6669.338149	26.547136
217.076950	6690.117600	26.552154
217.503157	6685.443083	26.557172
217.719287	6715.859995	26.562189
217.643368	6710.635301	26.567207
218.413872	6720.067088	26.572224
218.598323	6743.315276	26.577242
218.998158	6741.825103	26.582260
219.085684	6739.062138	26.587277
219.330868	6764.696419	26.592295
219.725624	6769.678314	26.597312
219.507938	6786.763312	26.602330
219.663443	6781.537108	26.607348
220.096291	6786.429538	26.612365
220.110458	6811.447696	26.617383
220.255300	6810.116966	26.622400
220.694733	6832.008365	26.627418
221.054381	6833.793672	26.632436
221.218832	6841.987758	26.637453
221.472538	6858.394237	26.642471
221.727803	6861.403900	26.647488
221.727966	6872.086039	26.652506
222.054865	6867.097632	26.657524
222.561479	6879.162469	26.662541
222.374506	6886.487337	26.667559
222.764303	6889.188385	26.672576
222.851612	6902.696953	26.677594
223.213228	6896.604649	26.682612
223.372595	6911.280345	26.687629
223.267810	6920.360826	26.692647
224.045606	6932.282559	26.697664
223.885810	6940.112960	26.702682
224.075685	6951.478535	26.707700
224.334069	6955.901581	26.712717
224.476069	6968.692594	26.717735
224.824415	6979.036853	26.722752
225.012756	6987.823600	26.727770
225.311590	6989.812958	26.732788
225.111524	6997.352401	26.737805
225.514659	7010.510172	26.742823
225.952216	7013.202057	26.747840
226.056489	7019.402661	26.752858
226.062368	7044.719154	26.757876
226.436839	7055.946020	26.762893
226.282609	7057.792023	26.767911
227.037566	7070.016491	26.772928
227.175959	7074.789940	26.777946
227.246277	7100.561254	26.782964
227.678315	7107.945709	26.787981
227.846402	7118.000932	26.792999
228.229800	7127.971488	26.798016
228.149244	7153.058035	26.803034
228.208023	7152.172160	26.808052
228.541806	7158.847659	26.813069
228.768050	7177.650743	26.818087
228.934732	7189.836110	26.823104
229.170671	7209.890277	26.828122
229.756454	7216.074797	26.833140
230.247119	7227.830889	26.838157
230.139609	7238.578449	26.843175
230.361628	7242.943648	26.848192
230.368207	7258.618106	26.853210
231.131262	7262.288871	26.858228
231.481522	7272.212090	26.863245
231.308134	7293.265554	26.868263
231.834210	7282.030273	26.873280
231.751071	7293.861356	26.878298
232.475789	7304.132477	26.883316
232.303230	7306.761945	26.888333
232.405939	7319.018200	26.893351
233.241508	7317.059608	26.898368
233.451247	7333.908728	26.903386
233.563746	7343.595297	26.908404
234.125363	7325.117242	26.913421
234.055225	7338.091882	26.918439
234.128397	7344.831037	26.923456
234.140454	7354.658725	26.928474
234.588575	7356.103471	26.933492
235.024320	7354.231422	26.938509
234.810237	7382.986509	26.943527
235.230066	7385.610478	26.948544
235.252872	7380.379252	26.953562
235.762734	7397.411930	26.958580
236.024528	7393.026197	26.963597
236.113575	7407.594785	26.968615
236.180753	7417.287053	26.973632
236.413442	7442.286393	26.978650
236.496992	7439.434236	26.983668
236.985075	7446.556575	26.988685
236.737231	7462.699042	26.993703
237.405175	7459.712032	26.998720
237.552408	7487.895939	27.003738
237.673091	7502.354144	27.008756
237.775951	7493.542684	27.013773
237.783475	7510.240121	27.018791
238.384293	7521.906504	27.023808
238.331588	7544.025324	27.028826
238.636123	7554.591773	27.033844
239.059678	7551.590982	27.038861
238.909116	7585.867688	27.043879
239.367338	7594.105066	27.048896
239.819715	7607.522254	27.053914
239.872238	7625.933432	27.058932
240.055401	7638.921465	27.063949
240.529061	7649.525545	27.068967
240.882471	7666.977671	27.073984
241.180438	7686.279832	27.079002
241.309570	7680.583848	27.084020
241.709352	7682.960069	27.089037
242.042735	7713.594816	27.094055
242.251832	7714.271197	27.099072
242.530954	7721.664600	27.104090
242.763077	7735.277524	27.109108
242.892592	7738.815705	27.114125
242.810078	7748.463594	27.119143
243.259664	7753.865124	27.124160
243.569027	7769.396654	27.129178
243.836422	7789.657463	27.134196
244.477202	7796.002635	27.139213
244.285560	7810.354341	27.144231
244.714798	7803.674931	27.149248
244.828319	7816.734018	27.154266
244.828126	7815.693842	27.159284
245.246979	7825.978675	27.164301
245.846958	7845.102292	27.169319
245.956748	7844.194869	27.174336
246.035666	7852.049073	27.179354
246.166957	7873.747998	27.184372
246.772026	7871.675796	27.189389
246.491030	7891.421434	27.194407
246.987899	7888.970695	27.199424
247.370277	7901.800525	27.204442
247.578537	7913.569131	27.209460
248.053623	7920.828323	27.214477
247.926768	7931.435474	27.219495
248.146960	7936.162330	27.224512
248.583796	7953.553893	27.229530
248.635095	7971.373202	27.234548
248.884857	7977.900377	27.239565
249.174363	7997.787344	27.244583
249.415285	7999.313180	27.249600
249.383349	8023.069972	27.254618
249.630275	8033.895377	27.259636
250.020516	8056.897230	27.264653
250.244097	8049.137888	27.269671
250.331063	8061.970877	27.274688
250.513847	8078.010751	27.279706
250.575242	8097.702876	27.284724
250.925163	8103.317134	27.289741
251.307774	8126.849861	27.294759
251.737078	8140.953413	27.299776
252.315479	8137.632759	27.304794
252.114300	8155.380796	27.309812
252.184553	8167.785345	27.314829
252.301819	8176.407872	27.319847
252.619073	8187.375616	27.324864
253.340176	8208.209904	27.329882
253.825626	8224.325232	27.334900
254.557757	8217.423468	27.339917
254.377537	8235.296517	27.344935
254.892411	8224.004880	27.349952
255.362976	8220.987025	27.354970
255.187563	8247.517106	27.359988
255.629302	8252.611624	27.365005
255.573234	8250.385086	27.370023
255.531196	8251.427280	27.375040
256.115836	8264.433704	27.380058
256.246983	8271.651106	27.385076
256.587606	8265.622972	27.390093
256.708588	8290.694264	27.395111
256.748305	8307.673095	27.400128
257.102657	8304.145762	27.405146
257.142019	8321.662878	27.410164
257.419947	8330.915343	27.415181
257.600651	8352.574043	27.420199
258.017018	8363.011512	27.425216
258.060223	8382.064044	27.430234
258.127421	8402.782506	27.435252
258.695325	8415.409314	27.440269
258.793326	8443.419540	27.445287
259.288278	8447.623566	27.450304
259.935938	8457.151601	27.455322
260.100542	8481.134316	27.460340
260.468890	8478.490729	27.465357
260.430504	8493.622058	27.470375
260.758457	8519.069920	27.475392
261.263204	8515.803417	27.480410
261.288678	8531.063096	27.485428
261.888902	8525.402657	27.490445
262.261610	8539.462889	27.495463
262.063319	8549.134468	27.500480
262.659651	8555.508303	27.505498
262.666968	8562.712533	27.510516
263.113491	8567.956693	27.515533
263.366547	8603.875779	27.520551
263.049660	8601.909509	27.525568
263.990630	8607.352645	27.530586
264.026827	8628.443046	27.535604
264.196579	8618.879023	27.540621
264.338434	8633.188594	27.545639
264.618454	8645.426339	27.550656
264.995007	8653.673395	27.555674
265.040644	8665.367009	27.560692
265.415025	8673.228063	27.565709
265.769073	8678.782081	27.570727
266.064609	8688.367175	27.575744
266.328681	8702.699039	27.580762
266.255552	8718.956654	27.585780
266.558765	8721.815849	27.590797
266.737946	8742.124280	27.595815
266.682988	8757.832943	27.600832
267.020813	8762.216333	27.605850
267.163888	8780.815162	27.610868
267.445822	8809.787450	27.615885
267.749544	8830.277595	27.620903
267.827304	8839.908906	27.625920
268.703626	8859.954124	27.630938
268.736204	8884.077351	27.635956
269.142528	8886.483026	27.640973
269.329888	8909.123908	27.645991
269.557446	8922.370776	27.651008
270.393336	8942.371796	27.656026
270.377351	8960.351733	27.661044
270.803695	8964.322907	27.666061
271.046878	8983.336465	27.671079
271.378593	8993.315734	27.676096
271.633996	8992.590023	27.681114
271.665871	9016.554229	27.686132
272.183763	9026.552242	27.691149
272.608243	9034.580982	27.696167
272.675860	9047.319936	27.701184
273.133199	9048.494665	27.706202
273.354998	9077.837458	27.711220
273.700001	9075.052700	27.716237
273.674770	9081.285429	27.721255
274.104534	9098.488246	27.726272
274.732847	9090.835407	27.731290
274.414830	9112.617582	27.736308
274.918330	9121.133853	27.741325
275.153227	9129.409259	27.746343
275.640403	9143.039089	27.751360
275.959219	9152.956388	27.756378
275.902149	9158.366399	27.761396
276.397071	9173.756118	27.766413
276.932703	9183.888333	27.771431
276.938156	9193.919341	27.776448
277.284374	9192.987930	27.781466
277.283200	9200.793051	27.786484
277.774639	9205.521939	27.791501
277.908435	9219.799914	27.796519
278.161080	9231.858762	27.801536
278.757830	9247.527027	27.806554
278.591178	9258.285464	27.811572
278.943694	9268.670797	27.816589
279.182281	9276.273281	27.821607
279.233794	9291.338367	27.826624
279.828820	9292.454190	27.831642
280.135267	9317.448861	27.836660
280.046653	9321.586403	27.841677
280.327082	9334.486446	27.846695
280.304701	9349.891904	27.851712
280.930908	9358.968714	27.856730
281.282390	9378.289726	27.861748
281.507264	9376.011161	27.866765
282.219017	9401.449727	27.871783
282.251727	9410.660502	27.876800
282.540057	9407.916587	27.881818
282.624142	9436.190182	27.886836
282.707356	9442.478569	27.891853
283.374143	9461.234005	27.896871
283.319786	9467.434551	27.901888
283.936836	9490.408771	27.906906
284.112795	9507.052481	27.911924
284.271020	9512.540051	27.916941
284.596469	9535.746134	27.921959
284.654174	9562.286246	27.926976
285.108013	9556.562197	27.931994
285.435573	9585.160830	27.937012
285.662335	9604.566147	27.942029
285.922835	9618.241196	27.947047
286.125332	9636.385431	27.952064
286.743986	9654.497203	27.957082
286.994346	9671.271673	27.962100
287.188646	9677.305195	27.967117
287.704158	9692.232207	27.972135
287.488663	9710.739035	27.977152
288.204077	9708.601012	27.982170
288.391227	9740.192604	27.987188
288.556247	9751.340007	27.992205
288.917964	9778.493078	27.997223
288.810565	9789.004403	28.002240
289.370101	9798.572929	28.007258
289.838556	9821.022843	28.012276
290.051236	9834.789520	28.017293
290.488745	9855.063016	28.022311
290.849765	9868.562132	28.027328
291.251450	9867.062327	28.032346
291.308813	9883.086752	28.037364
291.494157	9903.926967	28.042381
291.845319	9913.965138	28.047399
292.093334	9934.309075	28.052416
292.370074	9952.839270	28.057434
292.661644	9973.435619	28.062452
292.832009	9975.266049	28.067469
293.372270	9990.757200	28.072487
293.178714	10014.038082	28.077504
294.085311	10032.641913	28.082522
294.223557	10038.978834	28.087540
294.534682	10058.167080	28.092557
295.038475	10073.721577	28.097575
295.139105	10079.396780	28.102592
295.658145	10090.253110	28.107610
295.840116	10099.041142	28.112628
295.967642	10117.941975	28.117645
296.480793	10113.191568	28.122663
296.629852	10135.045584	28.127680
297.059906	10143.340818	28.132698
297.500261	10154.434019	28.137716
297.395416	10162.290788	28.142733
297.837338	10163.649859	28.147751
298.069451	10172.529100	28.152768
298.218988	10174.032351	28.157786
298.415612	10197.427221	28.162804
298.562160	10212.047226	28.167821
298.944583	10226.274341	28.172839
298.630761	10245.294069	28.177856
299.452317	10259.086475	28.182874
299.894406	10282.285752	28.187892
299.925152	10307.975655	28.192909
300.552583	10328.840050	28.197927
300.746279	10340.729367	28.202944
301.011905	10347.911391	28.207962
301.240001	10378.833995	28.212980
301.738451	10393.937170	28.217997
302.350754	10398.478378	28.223015
302.445655	10430.016478	28.228032
302.772397	10437.843172	28.233050
303.052742	10455.855194	28.238068
303.489678	10461.118086	28.243085
303.875260	10476.715846	28.248103
303.904034	10494.354450	28.253120
304.497718	10506.265935	28.258138
304.671578	10521.228158	28.263156
305.348408	10542.118032	28.268173
305.548797	10534.063238	28.273191
305.498441	10548.910908	28.278208
306.025806	10568.076759	28.283226
306.200044	10582.468029	28.288244
306.731457	10590.597441	28.293261
307.008721	10599.794763	28.298279
307.233730	10613.328820	28.303296
307.376949	10633.010454	28.308314
307.342385	10646.012982	28.313332
307.879270	10653.220392	28.318349
308.437745	10671.885225	28.323367
308.483632	10684.452748	28.328384
308.474648	10695.505027	28.333402
309.253668	10722.314714	28.338420
308.883352	10741.012353	28.343437
309.509270	10743.379804	28.348455
309.965985	10776.372383	28.353472
310.121121	10797.631823	28.358490
310.638656	10810.862488	28.363508
310.625194	10836.060597	28.368525
311.442345	10835.789492	28.373543
311.441698	10855.067793	28.378560
311.744781	10882.827178	28.383578
312.379157	10869.946835	28.388596
312.492633	10894.213078	28.393613
312.863031	10905.867704	28.398631
312.824157	10915.585438	28.403648
313.397666	10929.908692	28.408666
313.842720	10942.556053	28.413684
314.005610	10971.705354	28.418701
314.360622	10972.324015	28.423719
314.482412	10987.677877	28.428736
315.171485	10993.779467	28.433754
315.743709	11006.384581	28.438772
315.795846	11026.666382	28.443789
315.897069	11029.014005	28.448807
316.306104	11039.809073	28.453824
316.618290	11047.659264	28.458842
316.813239	11076.092994	28.463860
317.194744	11096.703312	28.468877
317.483977	11123.384001	28.473895
317.762575	11131.823942	28.478912
318.010424	11139.001703	28.483930
318.261373	11150.072312	28.488948
318.584555	11171.943768	28.493965
318.877532	11191.729370	28.498983
319.010861	11212.919681	28.504000
319.627090	11227.588208	28.509018
319.797558	11246.494832	28.514036
319.775542	11266.249667	28.519053
320.410980	11283.722081	28.524071
320.789939	11309.434936	28.529088
321.110076	11324.886605	28.534106
321.758375	11341.287084	28.539124
321.950230	11364.604648	28.544141
322.293320	11378.412562	28.549159
322.558618	11398.431083	28.554176
323.203762	11413.489090	28.559194
323.708230	11423.285841	28.564212
323.344456	11446.734967	28.569229
323.994821	11453.886120	28.574247
324.067097	11481.697950	28.579264
324.482063	11497.045750	28.584282
324.865260	11511.447111	28.589300
325.094533	11524.705849	28.594317
325.752183	11549.056822	28.599335
325.949427	11564.218624	28.604352
326.513261	11576.113686	28.609370
326.866646	11569.434093	28.614388
327.065546	11600.495688	28.619405
327.823905	11604.794417	28.624423
327.605722	11623.594826	28.629440
327.862629	11636.712315	28.634458
328.357353	11640.441933	28.639476
328.718314	11664.011229	28.644493
328.880625	11665.847089	28.649511
329.183324	11685.665241	28.654528
329.435095	11695.524083	28.659546
329.661711	11696.869606	28.664564
329.661218	11728.187544	28.669581
330.021432	11743.078394	28.674599
330.524573	11754.927390	28.679616
330.618772	11777.751939	28.684634
331.277393	11787.177278	28.689652
331.189198	11807.808327	28.694669
331.987494	11820.351344	28.699687
331.893299	11843.935604	28.704704
332.247290	11863.356229	28.709722
332.842614	11880.347763	28.714740
332.802480	11899.328709	28.719757
333.103162	11918.534771	28.724775
333.663498	11951.730641	28.729792
333.693198	11966.753478	28.734810
334.433751	11985.820272	28.739828
334.693538	12008.091849	28.744845
335.301391	12036.796091	28.749863
335.757115	12057.936608	28.754880
336.054388	12071.275896	28.759898
336.586690	12079.474064	28.764916
336.417811	12106.996482	28.769933
336.970281	12105.501762	28.774951
337.324184	12128.759463	28.779968
337.640166	12128.482033	28.784986
338.475120	12153.038703	28.790004
338.387376	12164.388933	28.795021
338.625814	12173.616824	28.800039
339.113631	12200.144992	28.805056
339.478210	12214.599579	28.810074
339.862561	12227.324206	28.815092
340.154181	12246.787533	28.820109
340.364257	12269.540642	28.825127
340.463262	12278.960429	28.830144
341.120857	12292.472715	28.835162
341.243855	12318.309147	28.840180
341.999627	12325.428972	28.845197
342.467318	12353.019621	28.850215
342.355339	12375.314774	28.855232
342.821358	12384.577170	28.860250
343.189462	12387.571564	28.865268
343.423898	12410.239540	28.870285
343.665325	12434.588813	28.875303
343.815444	12443.882103	28.880320
344.246463	12471.822175	28.885338
344.804102	12490.771968	28.890356
344.977018	12518.297337	28.895373
345.312693	12528.710251	28.900391
345.553107	12555.825882	28.905408
346.153654	12576.043823	28.910426
346.918732	12589.970179	28.915444
347.172004	12616.019337	28.920461
347.607695	12609.898782	28.925479
347.951780	12622.305684	28.930496
348.522902	12636.805883	28.935514
348.841020	12632.108021	28.940532
348.871211	12641.484691	28.945549
349.045415	12649.885254	28.950567
349.469898	12657.074361	28.955584
349.210646	12673.003443	28.960602
349.894559	12688.434358	28.965620
349.956611	12720.720374	28.970637
350.362561	12732.675753	28.975655
350.501752	12746.265741	28.980672
350.814981	12775.982330	28.985690
351.311793	12793.865451	28.990708
351.573028	12832.408072	28.995725
352.158981	12850.235734	29.000743
352.223450	12870.268925	29.005760
352.464469	12890.353901	29.010778
353.335857	12905.266378	29.015796
353.322457	12937.737252	29.020813
353.738834	12953.547950	29.025831
354.526543	12982.346154	29.030848
354.758721	13008.469401	29.035866
355.169671	13021.463980	29.040884
355.299116	13048.602111	29.045901
355.757537	13059.631424	29.050919
355.993761	13089.447086	29.055936
356.202821	13107.645622	29.060954
356.987111	13120.784070	29.065972
357.210908	13154.703877	29.070989
357.312618	13163.727275	29.076007
357.843767	13188.536529	29.081024
358.313750	13209.063814	29.086042
358.822318	13220.225951	29.091060
359.300337	13246.993654	29.096077
359.546517	13244.550555	29.101095
359.981924	13262.244088	29.106112
360.516414	13288.144118	29.111130
360.917029	13298.417144	29.116148
361.180047	13315.879835	29.121165
361.376618	13326.011439	29.126183
361.709560	13355.359617	29.131200
361.942492	13369.315210	29.136218
362.606101	13377.566175	29.141236
362.574688	13409.099523	29.146253
362.950715	13418.586077	29.151271
363.567881	13440.753229	29.156288
363.710587	13451.496047	29.161306
364.587798	13479.796066	29.166324
364.713458	13489.364866	29.171341
365.227405	13520.646644	29.176359
365.610508	13526.787807	29.181376
365.730979	13538.082861	29.186394
366.363465	13543.194867	29.191412
366.608071	13568.935141	29.196429
366.581834	13571.758634	29.201447
367.240675	13600.772186	29.206464
367.354178	13620.172385	29.211482
367.721901	13628.760499	29.216500
367.961521	13652.238882	29.221517
368.055944	13662.498563	29.226535
368.323493	13684.167042	29.231552
368.591640	13700.021031	29.236570
369.154860	13729.090603	29.241588
369.417957	13748.916196	29.246605
369.714105	13773.901211	29.251623
370.315642	13806.296028	29.256640
370.482841	13836.403001	29.261658
371.015688	13855.041728	29.266676
371.444184	13866.082598	29.271693
371.802889	13905.537707	29.276711
372.034674	13935.990379	29.281728
372.167934	13957.376802	29.286746
372.819894	13977.221220	29.291764
373.149400	14003.231585	29.296781
373.779435	14039.118127	29.301799
374.209271	14046.915719	29.306816
374.632013	14076.510252	29.311834
374.944175	14100.574338	29.316852
375.412249	14120.408909	29.321869
375.528340	14150.629437	29.326887
376.107261	14160.869130	29.331904
376.451922	14188.480462	29.336922
376.962959	14196.012315	29.341940
377.353306	14219.467066	29.346957
377.861673	14235.959911	29.351975
378.195845	14258.603047	29.356992
378.494348	14283.735331	29.362010
378.986594	14287.834709	29.367028
379.719841	14312.236054	29.372045
379.704333	14329.489441	29.377063
380.178542	14347.421788	29.382080
380.239122	14375.827819	29.387098
380.795377	14386.070981	29.392116
380.914306	14421.821224	29.397133
381.320222	14445.029028	29.402151
382.029198	14459.577894	29.407168
382.068486	14500.606370	29.412186
382.460807	14513.727508	29.417204
383.339325	14531.654889	29.422221
383.340022	14562.409044	29.427239
383.727795	14571.379532	29.432256
384.010852	14607.659616	29.437274
384.725931	14615.439606	29.442292
385.059257	14641.848181	29.447309
385.454615	14662.659429	29.452327
386.049358	14685.822656	29.457344
386.226282	14698.775375	29.462362
386.751220	14728.272433	29.467380
386.777760	14737.058511	29.472397
387.510745	14755.788178	29.477415
387.653808	14769.715884	29.482432
387.770244	14794.523090	29.487450
388.583444	14798.529751	29.492468
388.797778	14823.553532	29.497485
388.766826	14839.653066	29.502503
389.347593	14855.780120	29.507520
389.347558	14888.874415	29.512538
389.816816	14902.086952	29.517556
390.342660	14930.233413	29.522573
390.477837	14957.342123	29.527591
391.173604	14983.388992	29.532608
391.006904	15007.511716	29.537626
391.698300	15035.275979	29.542644
392.248181	15068.756946	29.547661
392.690313	15088.710641	29.552679
393.311743	15107.094527	29.557696
393.227726	15134.844359	29.562714
394.130617	15160.153184	29.567732
394.700639	15186.459355	29.572749
395.237437	15198.040899	29.577767
395.664678	15202.513303	29.582784
395.988620	15223.543143	29.587802
396.295341	15241.201035	29.592820
396.803932	15257.469809	29.597837
397.193739	15283.064871	29.602855
397.741879	15306.942904	29.607872
397.911075	15318.125631	29.612890
398.248654	15345.511890	29.617908
398.871843	15357.588734	29.622925
398.994469	15374.263834	29.627943
399.357989	15397.953952	29.632960
399.542112	15417.216076	29.637978
400.056393	15456.806476	29.642996
400.606745	15467.530541	29.648013
400.750789	15495.955956	29.653031
401.274320	15519.083874	29.658048
401.825850	15541.535951	29.663066
401.832087	15582.318016	29.668084
402.130949	15588.578243	29.673101
402.710317	15633.929099	29.678119
403.290282	15657.508870	29.683136
403.546839	15679.987186	29.688154
403.967625	15706.560993	29.693172
404.387590	15719.647180	29.698189
404.538277	15753.976067	29.703207
404.912432	15772.628652	29.708224
405.462386	15803.632072	29.713242
405.744112	15834.641092	29.718260
406.328128	15860.697620	29.723277
406.826895	15887.004050	29.728295
407.240606	15910.807612	29.733312
407.573753	15937.582165	29.738330
408.181274	15971.012429	29.743348
409.328554	15984.728502	29.748365
409.251289	16003.462342	29.753383
409.922885	16018.404715	29.758400
410.334750	16020.464102	29.763418
410.299469	16041.890427	29.768436
410.606331	16050.793002	29.773453
411.280123	16064.875084	29.778471
411.547153	16087.473863	29.783488
411.953610	16100.191333	29.788506
412.377758	16111.891997	29.793524
412.942189	16141.883832	29.798541
412.897819	16163.574131	29.803559
413.456756	16182.248359	29.808576
413.854493	16205.731258	29.813594
413.818325	16233.412960	29.818612
414.389132	16247.615539	29.823629
414.938255	16273.802326	29.828647
415.522396	16298.508224	29.833664
415.734934	16317.731918	29.838682
416.109077	16333.998068	29.843700
416.675710	16360.679774	29.848717
416.940057	16387.363038	29.853735
417.237353	16416.923536	29.858752
417.791017	16441.160969	29.863770
418.169546	16482.717479	29.868788
418.666612	16507.988490	29.873805
418.845410	16530.451606	29.878823
419.382783	16558.509772	29.883840
419.628293	16589.183417	29.888858
420.318044	16620.907650	29.893876
421.042868	16635.107900	29.898893
421.146891	16672.635792	29.903911
421.709429	16694.505407	29.908928
422.369001	16715.487662	29.913946
423.039921	16740.155253	29.918964
423.199557	16747.454639	29.923981
423.497666	16778.263570	29.928999
424.082423	16789.816937	29.934016
424.659622	16811.597977	29.939034
424.826681	16846.949006	29.944052
425.308570	16864.556062	29.949069
425.786120	16888.740983	29.954087
425.855393	16915.072429	29.959104
426.453354	16936.107710	29.964122
426.538396	16964.334535	29.969140
427.146133	16986.527838	29.974157
427.431567	17026.731514	29.979175
427.690157	17048.665015	29.984192
428.622744	17071.107640	29.989210
429.158204	17113.179177	29.994228
429.690353	17120.975044	29.999245
429.876145	17156.199794	30.004263
430.359939	17170.950503	30.009280
430.790710	17198.497939	30.014298
430.982198	17215.271239	30.019316
431.792033	17230.933550	30.024333
432.068598	17264.944206	30.029351
432.704246	17291.553549	30.034368
432.996896	17301.195955	30.039386
433.431819	17326.151274	30.044404
433.902877	17328.289990	30.049421
434.011328	17354.216570	30.054439
434.305858	17376.979383	30.059456
434.951189	17393.848474	30.064474
435.169373	17429.131083	30.069492
435.638994	17443.281608	30.074509
435.857791	17469.040225	30.079527
436.513585	17495.859095	30.084544
437.077585	17526.671450	30.089562
437.060034	17556.841531	30.094580
437.851828	17575.335589	30.099597
438.069137	17613.181552	30.104615
438.283540	17639.464736	30.109632
438.826964	17663.393744	30.114650
439.179258	17701.815817	30.119668
439.831777	17722.569291	30.124685
440.044541	17759.938219	30.129703
440.789861	17797.292669	30.134720
441.462682	17815.546931	30.139738
441.585008	17842.568312	30.144756
441.939187	17873.234087	30.149773
442.552655	17897.911312	30.154791
442.866554	17939.256661	30.159808
443.591088	17956.548179	30.164826
443.989515	17988.959405	30.169844
444.734986	18010.155326	30.174861
445.299391	18045.324345	30.179879
445.614972	18068.166708	30.184896
445.922528	18095.800726	30.189914
446.154414	18136.145930	30.194932
446.621923	18151.102725	30.199949
446.924768	18179.736816	30.204967
447.352683	18220.297458	30.209984
448.315719	18245.954949	30.215002
448.576419	18278.268647	30.220020
449.176288	18295.350492	30.225037
449.426261	18329.182100	30.230055
449.886866	18349.703810	30.235072
450.627002	18374.123043	30.240090
451.090121	18395.755409	30.245108
451.457716	18424.560736	30.250125
451.661575	18445.976211	30.255143
452.307561	18468.128749	30.260160
452.924649	18502.137287	30.265178
453.261476	18525.980862	30.270196
453.602980	18545.196629	30.275213
453.990287	18573.624689	30.280231
454.376385	18610.028893	30.285248
454.666463	18633.471422	30.290266
455.090431	18676.368905	30.295284
455.609930	18694.899027	30.300301
456.142783	18714.078222	30.305319
456.419644	18752.638737	30.310336
456.930149	18779.890464	30.315354
457.185871	18806.265108	30.320372
457.718340	18822.351973	30.325389
458.164157	18865.326812	30.330407
459.050087	18891.246482	30.335424
459.441683	18908.288562	30.340442
459.601667	18939.698806	30.345460
460.203343	18959.035061	30.350477
460.814810	18986.880525	30.355495
460.931564	19018.691522	30.360512
461.228044	19044.740781	30.365530
461.723345	19081.546813	30.370548
462.309604	19094.778092	30.375565
462.561673	19141.444478	30.380583
462.891979	19176.437997	30.385600
463.347389	19201.221618	30.390618
463.604081	19245.799727	30.395636
464.608289	19275.597382	30.400653
465.370570	19305.904122	30.405671
465.648083	19334.911714	30.410688
466.338586	19364.656360	30.415706
466.487521	19389.482015	30.420724
467.075308	19420.086469	30.425741
467.520482	19456.717114	30.430759
467.600833	19482.275527	30.435776
468.286803	19500.478901	30.440794
468.639590	19557.941236	30.445812
469.067999	19578.215752	30.450829
469.836468	19606.559788	30.455847
470.493203	19651.878527	30.460864
470.998689	19672.081830	30.465882
471.222615	19709.823966	30.470900
471.710235	19741.131664	30.475917
472.225007	19776.754276	30.480935
472.550450	19810.557398	30.485952
473.219958	19825.490330	30.490970
473.803313	19876.370212	30.495988
474.177199	19898.203942	30.501005
474.515337	19932.435652	30.506023
474.930381	19968.078523	30.511040
475.390675	19997.814985	30.516058
475.747727	20041.476949	30.521076
476.299950	20070.750444	30.526093
477.066733	20099.259047	30.531111
477.386789	20135.102486	30.536128
478.347952	20167.632180	30.541146
478.515707	20195.909185	30.546164
479.049856	20225.558325	30.551181
479.484908	20255.478843	30.556199
479.795372	20284.980246	30.561216
480.559701	20316.011535	30.566234
481.006953	20352.026568	30.571252
481.383044	20379.152495	30.576269
481.792608	20405.933731	30.581287
482.254760	20436.579884	30.586304
482.916175	20455.253301	30.591322
483.231415	20472.616380	30.596340
483.521452	20497.454001	30.601357
484.386085	20521.514231	30.606375
485.041824	20551.260384	30.611392
485.550606	20577.616222	30.616410
485.632328	20596.204174	30.621428
485.878727	20624.511163	30.626445
486.623332	20654.767043	30.631463
486.478394	20689.976682	30.636480
487.354444	20718.884026	30.641498
487.915490	20748.382614	30.646516
488.597896	20789.354351	30.651533
489.267085	20812.269633	30.656551
489.430527	20844.647851	30.661568
489.901890	20873.667982	30.666586
490.254371	20899.749220	30.671604
490.664892	20932.497768	30.676621
491.237177	20973.248518	30.681639
491.724738	21009.681147	30.686656
492.267634	21040.907440	30.691674
492.414830	21080.706741	30.696692
492.859848	21121.400971	30.701709
493.470840	21148.981048	30.706727
493.782843	21189.720268	30.711744
494.753691	21226.197305	30.716762
494.991219	21266.745406	30.721780
495.770170	21294.192670	30.726797
496.136317	21332.768172	30.731815
496.696056	21381.509906	30.736832
497.536559	21400.492602	30.741850
497.794690	21445.465399	30.746868
498.400007	21471.849895	30.751885
498.913377	21514.683448	30.756903
499.431625	21534.155508	30.761920
500.285975	21573.962734	30.766938
500.474819	21605.966755	30.771956
501.032671	21631.794412	30.776973
501.834357	21664.171103	30.781991
501.787048	21700.112077	30.787008
502.619105	21724.571554	30.792026
503.023220	21756.030473	30.797044
503.781278	21789.405899	30.802061
504.000908	21819.008927	30.807079
504.345904	21847.891904	30.812096
504.644059	21881.395908	30.817114
505.171068	21915.891297	30.822132
505.723449	21967.242843	30.827149
506.491001	22001.003901	30.832167
506.521079	22035.196734	30.837184
507.000500	22066.852198	30.842202
507.778432	22107.015539	30.847220
507.945482	22147.484203	30.852237
508.852446	22174.017941	30.857255
509.234114	22217.400485	30.862272
509.927514	22243.122500	30.867290
510.163953	22273.079688	30.872308
510.739611	22316.231561	30.877325
511.660715	22343.490269	30.882343
511.973215	22372.489647	30.887360
512.536598	22398.617754	30.892378
512.778611	22427.510322	30.897396
513.101200	22468.262981	30.902413
513.591877	22495.190416	30.907431
513.824281	22536.188378	30.912448
514.639281	22573.095046	30.917466
514.968674	22612.148156	30.922484
515.662834	22642.912098	30.927501
516.424385	22688.316260	30.932519
516.711716	22723.518690	30.937536
517.446706	22753.877820	30.942554
517.701836	22802.236140	30.947572
518.086806	22840.658757	30.952589
518.913328	22862.608431	30.957607
519.314650	22909.441828	30.962624
519.844790	22950.349337	30.967642
520.500552	22986.490788	30.972660
521.006715	23018.265197	30.977677
521.687495	23055.834705	30.982695
521.765297	23103.751983	30.987712
522.367982	23136.761208	30.992730
523.012345	23176.675249	30.997748
523.700612	23218.893289	31.002765
524.372905	23258.284043	31.007783
524.588443	23294.145032	31.012800
524.975693	23337.750301	31.017818
525.693783	23382.729399	31.022836
526.176402	23421.942836	31.027853
526.847435	23450.973729	31.032871
527.045553	23493.572233	31.037888
527.787704	23523.006230	31.042906
528.552693	23567.003285	31.047924
528.756874	23606.565556	31.052941
529.470653	23647.047860	31.057959
530.042621	23691.014566	31.062976
530.973550	23723.266217	31.067994
531.536489	23761.257873	31.073012
531.575879	23797.333940	31.078029
532.386425	23821.501592	31.083047
532.845618	23864.294232	31.088064
533.268428	23906.910045	31.093082
533.986960	23935.315164	31.098100
534.443092	23968.007622	31.103117
534.922797	24008.001972	31.108135
535.195159	24041.372097	31.113152
536.349440	24076.949079	31.118170
536.952021	24106.535570	31.123188
537.053225	24150.970788	31.128205
538.018482	24179.222839	31.133223
538.128700	24205.086625	31.138240
538.646331	24242.948021	31.143258
539.159688	24276.226696	31.148276
539.371441	24305.574911	31.153293
540.175596	24330.899098	31.158311
540.806873	24376.032688	31.163328
541.080989	24401.848637	31.168346
541.672276	24436.292034	31.173364
541.964082	24478.327667	31.178381
542.903952	24509.457833	31.183399
543.195113	24558.621575	31.188416
543.618232	24588.532932	31.193434
544.445458	24628.107220	31.198452
544.395436	24668.146638	31.203469
545.250991	24709.057275	31.208487
545.544359	24749.968543	31.213504
546.390141	24789.718298	31.218522
547.111015	24825.751965	31.223540
547.347823	24884.763797	31.228557
548.309956	24906.808153	31.233575
548.768579	24955.473036	31.238592
549.177974	24986.540535	31.243610
550.005580	25031.741609	31.248628
550.379165	25076.510192	31.253645
551.026528	25114.559385	31.258663
551.148769	25152.955399	31.263680
551.671872	25174.005837	31.268698
552.499152	25227.102849	31.273716
552.757329	25275.880194	31.278733
553.847675	25306.547623	31.283751
554.281546	25353.413766	31.288768
554.764137	25387.924588	31.293786
555.722480	25433.006726	31.298804
556.141715	25473.785583	31.303821
556.344403	25507.080074	31.308839
557.115087	25559.927255	31.313856
558.056235	25594.211098	31.318874
558.605864	25632.889957	31.323892
558.733350	25669.498985	31.328909
559.413683	25701.915101	31.333927
559.719764	25742.058834	31.338944
560.221341	25782.256610	31.343962
561.146951	25826.596712	31.348980
561.446912	25873.559756	31.353997
562.307716	25905.466226	31.359015
562.597496	25948.190614	31.364032
563.412300	25992.028112	31.369050
563.932036	26030.551992	31.374068
564.268177	26073.110990	31.379085
565.127065	26107.949446	31.384103
565.561851	26154.720110	31.389120
565.826528	26194.924353	31.394138
566.259153	26242.513324	31.399156
566.971207	26278.564287	31.404173
567.814633	26313.500187	31.409191
567.982393	26362.866382	31.414208
568.396939	26396.062809	31.419226
569.305614	26435.419068	31.424244
569.629094	26482.432932	31.429261
570.341272	26510.948445	31.434279
571.039056	26563.738866	31.439296
571.620049	26594.326823	31.444314
572.224607	26635.931519	31.449332
572.683716	26681.541003	31.454349
573.543108	26719.393243	31.459367
573.885333	26757.692682	31.464384
574.305920	26789.143199	31.469402
575.112079	26840.047820	31.474420
575.340495	26872.524887	31.479437
576.128736	26922.312365	31.484455
576.983446	26954.997893	31.489472
577.112399	27016.465932	31.494490
577.683611	27052.080984	31.499508
578.081228	27091.305957	31.504525
578.679754	27126.116403	31.509543
579.409955	27181.498764	31.514560
579.791214	27227.075713	31.519578
580.552831	27279.131162	31.524596
581.026854	27326.782144	31.529613
581.684708	27370.083538	31.534631
582.510483	27422.079600	31.539648
582.947773	27466.382259	31.544666
583.675324	27501.229696	31.549684
584.361519	27548.332302	31.554701
585.227907	27592.920716	31.559719
585.723156	27628.111103	31.564736
586.151517	27668.746763	31.569754
586.789313	27715.431343	31.574772
587.079254	27773.988390	31.579789
587.816019	27807.208115	31.584807
588.390515	27846.531241	31.589824
588.813932	27900.819394	31.594842
589.417203	27943.273837	31.599860
590.257245	27998.323223	31.604877
590.801015	28042.411968	31.609895
591.595235	28082.061520	31.614912
592.403220	28119.305987	31.619930
592.919831	28162.751761	31.624948
593.075928	28202.797889	31.629965
593.933468	28243.669984	31.634983
594.824220	28293.250777	31.640000
594.791978	28330.930502	31.645018
595.593108	28371.214693	31.650036
595.745518	28427.919285	31.655053
596.589641	28471.933011	31.660071
597.032004	28523.383862	31.665088
597.480663	28577.593057	31.670106
598.550338	28622.954808	31.675124
599.097797	28676.266164	31.680141
599.538911	28712.407493	31.685159
600.426737	28757.877371	31.690176
600.428046	28796.367519	31.695194
601.305931	28838.462275	31.700212
602.025660	28884.096372	31.705229
602.729777	28917.728568	31.710247
603.096488	28965.784398	31.715264
603.585566	28996.909215	31.720282
604.462503	29035.556750	31.725300
604.814696	29085.942735	31.730317
605.380635	29127.284246	31.735335
605.962600	29182.470162	31.740352
606.482737	29234.188232	31.745370
607.234075	29261.489783	31.750388
607.721588	29313.455981	31.755405
608.324699	29363.673652	31.760423
609.004892	29409.014536	31.765440
608.954631	29470.304541	31.770458
609.864610	29503.216522	31.775476
610.765669	29575.479476	31.780493
611.432964	29615.788080	31.785511
612.146610	29675.646088	31.790528
612.974102	29715.513398	31.795546
613.771104	29764.691293	31.800564
614.095094	29806.200709	31.805581
615.059235	29850.572563	31.810599
615.571579	29890.793059	31.815616
616.037727	29948.125911	31.820634
616.362811	29990.447216	31.825652
617.238765	30034.409694	31.830669
617.741281	30087.074107	31.835687
618.495600	30141.937988	31.840704
618.859023	30187.671886	31.845722
619.768874	30227.037225	31.850740
620.279043	30282.881291	31.855757
620.856596	30338.711667	31.860775
621.729232	30384.060876	31.865792
621.763321	30438.074380	31.870810
622.652959	30482.270708	31.875828
623.273167	30537.444101	31.880845
623.806585	30586.373322	31.885863
624.724100	30637.550333	31.890880
624.822013	30701.867729	31.895898
625.572582	30747.719638	31.900916
626.279277	30799.788063	31.905933
627.409269	30862.373643	31.910951
628.112027	30905.663159	31.915968
628.146387	30950.663591	31.920986
629.009898	31013.605808	31.926004
629.639675	31055.561428	31.931021
630.541716	31100.729861	31.936039
631.022354	31149.729063	31.941056
631.682074	31199.221563	31.946074
632.305127	31248.924935	31.951092
632.987886	31297.960168	31.956109
633.574135	31338.246541	31.961127
634.143791	31379.079391	31.966144
634.402089	31427.955648	31.971162
635.349530	31476.961882	31.976180
635.986929	31519.718117	31.981197
636.277336	31572.841903	31.986215
636.976360	31612.026661	31.991232
637.358288	31671.631175	31.996250
638.241843	31701.842547	32.001268
638.661360	31757.392445	32.006285
639.296183	31806.539279	32.011303
640.231191	31855.988357	32.016320
640.615164	31921.120807	32.021338
641.199665	31953.041468	32.026356
641.854011	32020.599437	32.031373
642.559557	32081.933338	32.036391
643.363717	32126.708826	32.041408
643.927152	32185.647977	32.046426
644.760032	32237.355715	32.051444
645.130869	32292.891533	32.056461
645.813402	32344.837902	32.061479
646.532838	32393.772854	32.066496
646.917654	32440.437988	32.071514
647.795453	32508.997916	32.076532
648.461987	32569.216050	32.081549
649.087943	32612.191313	32.086567
649.784628	32680.864332	32.091584
650.320596	32747.020852	32.096602
651.336620	32788.252688	32.101620
651.676806	32854.585821	32.106637
652.395481	32905.956052	32.111655
653.476490	32945.935898	32.116672
653.795860	33009.372767	32.121690
654.651034	33056.929394	32.126708
655.566658	33110.090999	32.131725
655.968774	33167.495749	32.136743
656.703466	33214.318582	32.141760
656.985078	33272.237816	32.146778
657.680663	33324.193079	32.151796
658.265842	33387.196596	32.156813
659.072478	33446.829761	32.161831
660.050528	33501.417072	32.166848
660.312672	33548.246734	32.171866
660.870331	33603.755646	32.176884
661.596368	33658.815496	32.181901
661.982306	33723.540196	32.186919
662.834053	33778.837364	32.191936
663.451230	33845.068897	32.196954
664.247307	33901.068901	32.201972
665.057236	33966.844635	32.206989
665.619586	34015.279777	32.212007
666.641962	34054.459860	32.217024
667.204546	34130.847885	32.222042
667.734513	34181.610573	32.227060
668.516231	34229.880583	32.232077
668.935816	34287.953222	32.237095
669.883914	34340.055905	32.242112
670.201946	34387.135982	32.247130
670.898930	34440.778055	32.252148
671.734249	34492.760458	32.257165
672.414900	34539.173189	32.262183
672.950112	34590.636193	32.267200
673.391587	34647.555867	32.272218
673.920567	34688.783302	32.277236
675.097380	34751.223330	32.282253
675.448772	34809.299190	32.287271
675.747939	34860.378143	32.292288
676.343909	34910.856687	32.297306
677.341109	34973.549995	32.302324
677.971646	35043.031545	32.307341
678.339392	35103.412095	32.312359
679.310393	35165.221207	32.317376
679.700727	35229.528601	32.322394
680.166475	35298.927105	32.327412
681.273837	35355.946548	32.332429
681.560241	35427.615817	32.337447
682.962670	35484.246638	32.342464
683.490031	35563.673614	32.347482
684.354957	35610.304349	32.352500
685.331824	35676.832740	32.357517
685.674493	35730.945264	32.362535
686.862949	35779.609047	32.367552
687.353152	35852.605033	32.372570
688.004711	35916.157767	32.377588
689.032686	35959.437154	32.382605
689.564231	36014.108555	32.387623
690.178696	36061.280173	32.392640
690.529146	36123.314601	32.397658
691.796348	36186.866522	32.402676
692.457725	36235.579290	32.407693
692.980314	36293.998816	32.412711
693.962798	36350.890202	32.417728
694.667815	36406.104391	32.422746
694.810410	36459.445522	32.427764
696.145455	36508.876365	32.432781
696.679803	36570.422826	32.437799
697.457007	36628.273267	32.442816
698.114730	36673.954623	32.447834
698.658849	36724.402769	32.452852
699.492578	36785.235477	32.457869
699.951670	36831.611041	32.462887
701.042441	36889.423501	32.467904
701.180048	36958.950506	32.472922
702.106926	37010.355471	32.477940
702.900026	37058.940884	32.482957
703.647006	37124.494741	32.487975
704.325457	37184.355635	32.492992
705.072669	37238.495343	32.498010
705.634064	37291.121309	32.503028
706.312175	37345.360652	32.508045
706.585041	37397.028580	32.513063
707.698396	37449.018509	32.518080
708.269770	37500.081109	32.523098
708.880424	37563.015955	32.528116
709.614666	37606.079921	32.533133
710.032435	37670.819593	32.538151
710.774875	37710.089119	32.543168
711.195059	37777.329378	32.548186
711.936911	37834.730802	32.553204
712.874252	37892.558534	32.558221
713.403317	37962.224448	32.563239
714.295314	38007.541041	32.568256
715.162734	38077.796854	32.573274
715.825143	38137.446114	32.578292
716.477260	38194.233952	32.583309
716.869782	38259.109191	32.588327
717.690317	38322.888533	32.593344
718.331737	38394.668475	32.598362
718.982243	38456.378364	32.603380
719.765720	38518.480413	32.608397
720.345265	38589.250893	32.613415
721.615234	38650.306295	32.618432
722.633575	38711.066129	32.623450
723.066384	38776.476187	32.628468
723.848296	38837.296187	32.633485
724.312794	38907.625902	32.638503
725.579676	38975.880876	32.643520
726.074591	39034.601297	32.648538
726.820361	39093.589459	32.653556
727.379952	39155.258033	32.658573
728.162623	39212.507853	32.663591
728.766629	39277.052166	32.668608
729.745424	39347.353872	32.673626
730.499324	39410.059935	32.678644
731.115789	39471.747413	32.683661
732.048600	39542.817274	32.688679
732.852766	39599.549363	32.693696
733.592334	39654.456498	32.698714
733.902777	39723.147413	32.703732
735.227350	39780.462691	32.708749
735.365854	39846.242247	32.713767
736.187356	39909.978538	32.718784
737.470384	39966.265067	32.723802
737.911713	40028.698341	32.728820
738.799140	40087.361502	32.733837
739.349100	40161.244953	32.738855
740.379605	40228.419871	32.743872
740.912871	40284.522468	32.748890
741.243733	40351.851819	32.753908
742.473777	40415.864008	32.758925
742.922745	40487.678716	32.763943
743.685660	40547.930730	32.768960
744.400538	40605.877268	32.773978
745.048831	40674.847819	32.778996
745.810713	40746.533385	32.784013
746.346191	40811.633743	32.789031
747.519292	40874.592293	32.794048
747.917642	40934.490546	32.799066
748.562853	40998.311015	32.804084
749.514106	41057.645451	32.809101
749.800808	41118.054130	32.814119
750.405537	41189.056937	32.819136
751.694017	41247.155627	32.824154
752.104923	41321.293321	32.829172
753.117516	41383.760474	32.834189
753.751569	41452.217604	32.839207
754.172201	41523.941828	32.844224
755.003755	41584.953000	32.849242
755.523162	41660.923145	32.854260
756.734703	41723.637427	32.859277
757.471063	41800.863660	32.864295
757.979801	41877.009933	32.869312
758.631877	41942.823049	32.874330
759.572353	42014.911307	32.879348
760.605942	42087.521245	32.884365
761.647958	42151.071530	32.889383
762.332988	42222.390713	32.894400
763.399521	42290.678268	32.899418
764.062504	42364.635260	32.904436
764.844484	42413.441240	32.909453
765.501061	42481.110353	32.914471
766.103446	42547.167106	32.919488
766.887812	42619.465697	32.924506
767.792762	42694.994238	32.929524
768.761225	42759.261874	32.934541
769.487191	42825.259020	32.939559
770.583791	42888.718185	32.944576
771.532513	42953.377662	32.949594
771.710142	43014.135264	32.954612
772.421419	43074.095271	32.959629
773.312938	43138.020135	32.964647
774.361840	43213.464956	32.969664
775.227798	43281.662203	32.974682
775.722399	43347.329120	32.979700
776.229003	43409.590838	32.984717
777.162044	43479.604558	32.989735
778.244604	43547.200596	32.994752
778.888226	43614.907770	32.999770
779.237576	43679.021876	33.004788
780.474422	43740.692246	33.009805
781.262896	43825.379444	33.014823
781.735605	43895.931820	33.019840
782.670400	43955.963413	33.024858
783.461860	44018.907510	33.029876
784.058991	44088.138077	33.034893
784.974351	44173.948703	33.039911
785.748622	44232.174050	33.044928
786.853322	44300.819962	33.049946
787.129915	44385.310620	33.054964
788.010669	44447.238925	33.059981
788.604797	44513.664135	33.064999
789.348909	44572.053152	33.070016
790.112104	44640.944041	33.075034
790.744028	44711.695217	33.080052
791.555877	44772.152997	33.085069
792.329378	44847.617239	33.090087
793.182491	44916.999649	33.095104
794.080320	44981.447686	33.100122
794.923159	45052.867012	33.105140
795.452889	45115.929307	33.110157
796.322812	45190.663586	33.115175
797.033086	45262.215285	33.120192
797.942344	45325.400906	33.125210
798.834388	45393.741131	33.130228
799.702881	45469.448485	33.135245
800.420180	45540.239921	33.140263
801.129697	45611.742701	33.145280
801.908869	45689.793431	33.150298
802.456864	45764.641352	33.155316
803.830332	45830.272435	33.160333
804.562136	45907.451493	33.165351
805.287382	45993.342375	33.170368
806.242500	46047.487936	33.175386
807.050876	46117.058922	33.180404
808.349259	46188.142242	33.185421
808.982727	46260.394865	33.190439
809.064985	46325.337332	33.195456
810.608161	46398.764482	33.200474
811.152920	46476.111482	33.205492
811.753697	46548.651285	33.210509
812.827617	46616.251190	33.215527
813.332152	46699.133008	33.220544
814.408431	46771.803129	33.225562
815.067761	46840.640372	33.230580
816.211126	46917.619572	33.235597
816.990251	46995.890682	33.240615
817.770663	47061.131757	33.245632
818.941451	47134.785327	33.250650
819.056573	47209.074160	33.255668
820.031685	47281.128334	33.260685
820.911773	47357.974686	33.265703
821.865108	47434.715066	33.270720
822.730941	47504.847181	33.275738
823.546353	47578.707461	33.280756
824.481137	47651.558350	33.285773
825.434854	47724.065774	33.290791
826.026308	47803.449403	33.295808
827.449496	47863.126465	33.300826
828.007510	47941.452754	33.305844
828.480642	48014.116735	33.310861
829.347928	48089.510632	33.315879
829.867165	48168.705468	33.320896
831.102719	48240.491798	33.325914
831.921636	48315.285402	33.330932
832.484314	48374.258699	33.335949
833.332923	48454.588771	33.340967
833.955629	48531.030005	33.345984
834.946078	48589.882306	33.351002
835.815384	48670.910542	33.356020
836.477668	48740.379496	33.361037
837.544309	48807.017160	33.366055
838.111775	48866.168036	33.371072
838.825135	48934.651474	33.376090
839.461144	49004.532687	33.381108
840.389276	49069.167646	33.386125
841.569358	49161.097790	33.391143
841.969154	49241.471309	33.396160
842.974508	49313.566850	33.401178
843.745756	49399.107327	33.406196
844.603736	49466.591628	33.411213
845.628954	49546.816515	33.416231
846.238528	49619.844035	33.421248
847.341318	49697.138455	33.426266
848.368729	49782.699973	33.431284
849.206586	49854.849615	33.436301
850.462258	49928.482420	33.441319
850.861975	50006.559043	33.446336
852.221969	50076.168336	33.451354
852.959901	50148.208850	33.456372
853.767348	50214.732126	33.461389
854.945951	50286.920811	33.466407
855.729033	50364.505684	33.471424
856.764458	50424.477166	33.476442
857.200978	50507.201490	33.481460
858.124364	50573.070222	33.486477
858.725368	50640.697702	33.491495
859.317236	50734.493604	33.496512
860.670519	50795.927318	33.501530
861.714053	50874.482781	33.506548
862.548440	50954.491935	33.511565
863.372169	51027.248162	33.516583
864.002461	51096.131837	33.521600
865.212373	51180.178376	33.526618
865.804522	51260.044413	33.531636
866.527723	51333.581577	33.536653
867.605397	51403.613372	33.541671
868.076681	51492.875499	33.546688
868.742491	51575.757630	33.551706
869.807863	51659.529622	33.556724
870.649700	51736.962786	33.561741
871.449125	51815.820010	33.566759
872.323717	51912.650898	33.571776
873.096925	51994.277618	33.576794
873.770568	52081.355007	33.581812
874.994075	52180.688097	33.586829
876.033339	52259.736334	33.591847
876.869727	52339.331621	33.596864
877.842319	52426.994303	33.601882
878.717042	52507.679353	33.606900
879.226762	52600.393503	33.611917
880.161922	52673.324887	33.616935
881.079268	52753.537169	33.621952
882.129041	52837.692709	33.626970
882.594071	52918.037662	33.631988
883.479520	52984.988050	33.637005
884.514279	53047.556402	33.642023
884.935844	53138.311649	33.647040
886.359456	53213.158985	33.652058
887.121987	53292.612435	33.657076
887.756536	53381.119424	33.662093
889.060444	53466.070678	33.667111
889.362245	53547.280782	33.672128
890.540031	53621.225239	33.677146
891.375955	53714.000515	33.682164
892.036602	53809.834107	33.687181
893.089335	53883.487073	33.692199
893.769572	53981.698241	33.697216
894.660338	54076.458228	33.702234
895.600342	54166.880487	33.707252
896.198744	54259.690039	33.712269
897.577343	54342.540917	33.717287
898.228945	54439.805923	33.722304
899.356387	54527.299507	33.727322
900.406033	54622.980812	33.732340
901.338030	54719.438866	33.737357
902.433241	54794.180876	33.742375
903.035622	54890.875356	33.747392
904.167560	54987.647066	33.752410
905.137862	55072.952489	33.757428
906.439337	55160.639227	33.762445
907.378485	55242.020641	33.767463
908.073371	55331.105173	33.772480
909.381336	55409.007045	33.777498
910.158692	55495.806598	33.782516
910.836190	55590.305390	33.787533
911.991499	55656.092685	33.792551
912.675018	55750.114712	33.797568
913.590995	55835.858483	33.802586
914.871673	55916.361552	33.807604
915.642823	56003.372839	33.812621
916.342692	56088.063159	33.817639
917.444674	56174.321859	33.822656
918.493981	56257.811519	33.827674
919.037366	56358.961375	33.832692
919.691532	56443.278657	33.837709
921.408422	56515.706533	33.842727
921.870061	56605.127957	33.847744
922.766441	56689.234216	33.852762
923.623496	56783.622215	33.857780
924.367853	56877.413069	33.862797
925.450065	56957.368303	33.867815
926.259069	57055.550282	33.872832
927.563209	57148.786258	33.877850
928.342131	57236.474556	33.882868
929.102840	57328.342625	33.887885
930.444740	57410.645063	33.892903
931.162882	57497.987557	33.897920
931.781445	57577.788811	33.902938
932.792204	57651.447895	33.907956
933.874032	57725.316948	33.912973
934.848795	57806.072719	33.917991
935.313805	57888.620988	33.923008
936.657465	57960.343673	33.928026
937.351723	58047.559982	33.933044
938.254509	58140.012468	33.938061
939.286897	58221.051328	33.943079
939.986802	58311.447043	33.948096
940.650432	58405.028061	33.953114
941.620181	58487.915426	33.958132
942.609133	58578.708442	33.963149
943.542042	58677.365525	33.968167
944.354089	58780.989467	33.973184
945.427917	58870.832767	33.978202
946.449613	58968.163933	33.983220
946.886801	59075.059914	33.988237
948.126237	59169.872857	33.993255
948.995650	59272.322282	33.998272
950.127396	59366.338821	34.003290
951.071028	59469.800447	34.008308
952.117647	59563.351637	34.013325
953.252826	59663.923458	34.018343
954.035110	59764.652998	34.023360
955.241316	59863.683348	34.028378
956.383370	59958.815750	34.033396
957.120186	60056.330545	34.038413
958.514912	60154.009552	34.043431
959.382270	60244.274377	34.048448
960.202353	60332.804319	34.053466
961.235048	60434.624805	34.058484
962.193142	60525.555382	34.063501
963.317506	60614.293998	34.068519
964.110490	60700.146235	34.073536
965.365602	60797.986595	34.078554
966.651081	60885.598938	34.083572
967.180850	60982.447406	34.088589
968.549228	61066.574241	34.093607
969.431266	61154.438315	34.098624
970.373054	61246.742174	34.103642
971.703470	61333.560100	34.108660
972.477733	61432.446467	34.113677
973.447631	61516.727129	34.118695
974.077310	61610.853798	34.123712
975.270770	61702.365213	34.128730
976.448883	61795.562497	34.133748
976.444444	61885.430825	34.138765
977.952898	61978.860649	34.143783
978.970367	62080.547257	34.148800
979.926115	62175.862668	34.153818
980.625965	62269.792015	34.158836
981.539084	62367.432887	34.163853
982.924412	62461.888836	34.168871
984.069152	62539.161493	34.173888
984.621934	62622.847197	34.178906
985.871614	62695.935637	34.183924
986.473734	62793.685030	34.188941
987.373000	62874.146368	34.193959
987.942569	62966.341046	34.198976
988.613960	63063.992399	34.203994
989.934681	63158.398960	34.209012
991.013973	63273.262791	34.214029
991.925526	63356.127321	34.219047
993.128557	63463.005431	34.224064
993.675693	63552.844468	34.229082
994.901176	63657.800128	34.234100
995.681665	63757.967163	34.239117
997.266090	63860.615273	34.244135
998.166114	63959.785406	34.249152
998.961089	64050.989495	34.254170
1000.061436	64149.494008	34.259188
1001.114893	64253.681368	34.264205
1002.403532	64345.092558	34.269223
1003.646446	64440.424229	34.274240
1004.558973	64547.863100	34.279258
1005.616697	64635.159619	34.284276
1006.401776	64740.197635	34.289293
1007.503481	64841.064580	34.294311
1008.391136	64928.253698	34.299328
1009.186914	65028.829227	34.304346
1010.451658	65137.453371	34.309364
1011.486993	65242.094315	34.314381
1012.563918	65328.146647	34.319399
1013.648879	65438.430707	34.324416
1014.381570	65533.485816	34.329434
1015.443486	65643.550493	34.334452
1016.370673	65748.037708	34.339469
1017.249455	65851.854172	34.344487
1018.148135	65957.607201	34.349504
1019.361968	66058.383780	34.354522
1020.770618	66167.499365	34.359540
1021.821245	66276.249306	34.364557
1022.687280	66376.615450	34.369575
1023.628411	66492.755563	34.374592
1024.581030	66601.987214	34.379610
1025.905267	66700.292398	34.384628
1026.879256	66804.316796	34.389645
1027.696486	66910.827091	34.394663
1028.524313	67003.139159	34.399680
1029.725150	67110.808696	34.404698
1031.125720	67221.861362	34.409716
1032.175510	67325.848092	34.414733
1033.463375	67429.415337	34.419751
1034.668393	67526.505573	34.424768
1035.380492	67628.279833	34.429786
1036.762030	67731.249470	34.434804
1037.534010	67824.986222	34.439821
1038.409526	67928.435375	34.444839
1039.682488	68012.112247	34.449856
1040.628312	68097.900925	34.454874
1041.290615	68193.122496	34.459892
1042.341741	68278.560412	34.464909
1043.361438	68364.123732	34.469927
1044.494228	68471.464223	34.474944
1044.998934	68572.897392	34.479962
1046.379133	68653.382345	34.484980
1047.443671	68758.669493	34.489997
1048.250258	68856.840560	34.495015
1049.357410	68956.202544	34.500032
1050.333163	69064.013510	34.505050
1051.145399	69171.547837	34.510068
1052.124358	69280.692496	34.515085
1053.487640	69383.844388	34.520103
1054.266030	69491.480628	34.525120
1054.779978	69604.276855	34.530138
1056.431669	69717.227615	34.535156
1057.426617	69829.980231	34.540173
1058.309627	69950.680150	34.545191
1059.369064	70061.389509	34.550208
1060.398290	70174.075479	34.555226
1061.630875	70281.018356	34.560244
1062.540282	70407.434608	34.565261
1063.942333	70518.666995	34.570279
1065.104883	70641.683324	34.575296
1066.122365	70763.598880	34.580314
1067.464534	70863.185909	34.585332
1068.509054	70991.682045	34.590349
1069.187906	71087.370004	34.595367
1070.616050	71210.404518	34.600384
1071.602774	71311.111809	34.605402
1072.433889	71434.697592	34.610420
1073.460985	71552.016794	34.615437
1075.257392	71679.974513	34.620455
1076.659305	71771.273266	34.625472
1077.320741	71884.779428	34.630490
1078.813649	71999.316601	34.635508
1079.778114	72101.143519	34.640525
1080.786009	72217.408222	34.645543
1082.052907	72319.579915	34.650560
1083.012317	72432.808046	34.655578
1084.229317	72527.299008	34.660596
1085.169890	72643.172527	34.665613
1086.286602	72735.968074	34.670631
1087.312850	72849.813509	34.675648
1088.096684	72958.181862	34.680666
1089.561131	73072.837197	34.685684
1090.546455	73184.542666	34.690701
1091.618855	73288.386868	34.695719
1093.016050	73413.038691	34.700736
1093.780889	73513.211138	34.705754
1094.719999	73617.836532	34.710772
1095.856108	73733.224025	34.715789
1096.863411	73843.185646	34.720807
1098.100895	73943.266133	34.725824
1098.844203	74058.212448	34.730842
1100.368045	74137.388963	34.735860
1101.351808	74250.977447	34.740877
1102.054862	74340.528695	34.745895
1103.247606	74439.342304	34.750912
1104.300168	74556.131755	34.755930
1105.299611	74667.615793	34.760948
1106.221894	74772.565878	34.765965
1107.198178	74892.004586	34.770983
1108.301120	74994.241364	34.776000
1109.377016	75130.064538	34.781018
1110.540407	75245.683922	34.786036
1111.429980	75365.069719	34.791053
1112.460176	75479.435084	34.796071
1113.998377	75597.606870	34.801088
1114.905825	75728.841247	34.806106
1116.361349	75843.305354	34.811124
1117.376865	75962.074296	34.816141
1118.241325	76084.400702	34.821159
1120.129774	76196.131032	34.826176
1120.668066	76322.504859	34.831194
1122.001479	76440.587762	34.836212
1123.332717	76553.344021	34.841229
1124.410551	76677.795178	34.846247
1125.514084	76792.339604	34.851264
1126.819544	76903.465042	34.856282
1128.289561	77019.646241	34.861300
1129.073237	77134.224505	34.866317
1130.570022	77235.202886	34.871335
1132.461463	77334.039685	34.876352
1133.766551	77452.632291	34.881370
1134.859966	77546.825291	34.886388
1136.183787	77642.012289	34.891405
1137.012588	77760.537064	34.896423
1138.370570	77853.393758	34.901440
1139.029454	77963.894666	34.906458
1140.054438	78053.790424	34.911476
1140.917465	78176.685875	34.916493
1142.228707	78287.944380	34.921511
1143.498890	78392.895867	34.926528
1144.525027	78503.948068	34.931546
1145.055315	78625.337963	34.936564
1146.337798	78735.162396	34.941581
1147.320162	78859.471430	34.946599
1148.563627	78967.318640	34.951616
1149.348045	79100.737073	34.956634
1150.634457	79218.262080	34.961652
1152.240616	79344.725049	34.966669
1153.291000	79466.700909	34.971687
1154.562890	79592.706575	34.976704
1155.687372	79709.274093	34.981722
1156.715098	79824.252145	34.986740
1158.130775	79936.855684	34.991757
1159.249115	80054.134081	34.996775
1160.353921	80153.646912	35.001792
1161.490136	80269.191733	35.006810
1162.420966	80359.378067	35.011828
1163.798619	80474.114476	35.016845
1164.760141	80586.989740	35.021863
1166.199255	80671.635148	35.026880
1167.028581	80800.183833	35.031898
1168.210873	80902.210121	35.036916
1169.240221	81010.569867	35.041933
1169.915366	81127.577164	35.046951
1171.266413	81241.373869	35.051968
1172.398159	81363.227906	35.056986
1173.670777	81471.759991	35.062004
1174.875614	81603.338805	35.067021
1176.229421	81730.330646	35.072039
1177.374119	81844.365759	35.077056
1178.366546	81961.845677	35.082074
1179.397197	82094.302386	35.087092
1180.973187	82217.020076	35.092109
1181.878111	82336.184934	35.097127
1183.022373	82458.991659	35.102144
1184.194909	82590.240478	35.107162
1185.547678	82714.640249	35.112180
1186.841477	82834.523705	35.117197
1187.905314	82975.489922	35.122215
1189.514958	83083.825105	35.127232
1190.497435	83223.326602	35.132250
1191.590679	83343.877061	35.137268
1192.993337	83463.228411	35.142285
1194.307326	83586.615369	35.147303
1195.782147	83709.098710	35.152320
1196.624315	83833.333430	35.157338
1197.778595	83961.559128	35.162356
1199.172816	84090.095182	35.167373
1199.857213	84218.675331	35.172391
1201.282341	84337.484367	35.177408
1202.560149	84472.584831	35.182426
1203.893283	84601.715376	35.187444
1205.103587	84726.706100	35.192461
1206.603013	84863.999323	35.197479
1207.509001	84984.936695	35.202496
1208.800122	85113.558608	35.207514
1210.072183	85237.101001	35.212532
1211.532930	85369.459422	35.217549
1212.522804	85505.446852	35.222567
1213.918724	85612.513938	35.227584
1215.216927	85750.894471	35.232602
1216.371092	85872.151525	35.237620
1217.312637	86000.492972	35.242637
1218.681990	86118.239690	35.247655
1219.948606	86238.450338	35.252672
1220.625010	86381.802430	35.257690
1222.025608	86512.811800	35.262708
1223.326009	86636.876315	35.267725
1224.445782	86773.907141	35.272743
1225.651088	86887.011489	35.277760
1226.851468	87007.597420	35.282778
1228.141995	87126.310705	35.287796
1229.207204	87232.395208	35.292813
1230.583402	87365.923983	35.297831
1231.885927	87475.784846	35.302848
1232.840976	87591.885652	35.307866
1233.875479	87729.726565	35.312884
1235.058845	87845.937885	35.317901
1236.033385	87982.594846	35.322919
1237.229043	88108.638470	35.327936
1238.705792	88238.255154	35.332954
1239.657431	88371.345483	35.337972
1240.959014	88509.970994	35.342989
1242.042161	88647.133439	35.348007
1243.468608	88790.641666	35.353024
1244.553587	88928.153404	35.358042
1245.820124	89074.231043	35.363060
1247.154086	89201.593371	35.368077
1248.512311	89355.866530	35.373095
1249.726912	89487.385261	35.378112
1251.012205	89627.373829	35.383130
1252.309878	89769.637933	35.388148
1253.398272	89915.692653	35.393165
1254.977877	90056.623739	35.398183
1256.235426	90199.801368	35.403200
1257.302576	90345.343784	35.408218
1259.078503	90486.777673	35.413236
1260.469062	90625.636576	35.418253
1261.209495	90781.731913	35.423271
1262.739378	90923.372178	35.428288
1264.042260	91067.206022	35.433306
1265.268608	91201.560198	35.438324
1266.764270	91343.828412	35.443341
1267.853974	91486.864091	35.448359
1269.225678	91621.071250	35.453376
1270.585676	91769.947526	35.458394
1271.732518	91905.577230	35.463412
1273.189341	92045.623626	35.468429
1274.752847	92187.848590	35.473447
1276.328649	92325.689553	35.478464
1277.855382	92448.284093	35.483482
1278.867852	92591.054632	35.488500
1280.165705	92723.610548	35.493517
1281.373456	92854.866029	35.498535
1282.942679	92992.914609	35.503552
1284.291861	93124.414856	35.508570
1285.262351	93265.969412	35.513588
1286.478050	93385.260084	35.518605
1287.518555	93521.517505	35.523623
1288.876758	93660.445019	35.528640
1289.950253	93797.438919	35.533658
1291.510570	93941.731335	35.538676
1292.955915	94076.036613	35.543693
1293.994209	94210.167049	35.548711
1295.496071	94328.740519	35.553728
1296.691062	94450.507039	35.558746
1297.520940	94576.532238	35.563764
1298.686873	94691.663166	35.568781
1300.047456	94826.555726	35.573799
1301.266333	94953.001948	35.578816
1302.626772	95086.302108	35.583834
1303.520757	95216.647314	35.588852
1305.047890	95362.023211	35.593869
1306.081041	95501.013878	35.598887
1307.494846	95638.856906	35.603904
1308.759530	95779.476123	35.608922
1309.839993	95922.877160	35.613940
1311.547523	96058.424151	35.618957
1312.855737	96210.438039	35.623975
1314.150594	96354.269531	35.628992
1315.769089	96485.076271	35.634010
1316.847704	96636.319827	35.639028
1318.311689	96777.463959	35.644045
1319.370866	96932.843398	35.649063
1320.836922	97070.895656	35.654080
1322.267372	97220.878948	35.659098
1323.411841	97364.563657	35.664116
1324.500367	97506.461559	35.669133
1326.170588	97675.350080	35.674151
1327.200476	97815.854836	35.679168
1328.712288	97964.488971	35.684186
1330.127684	98123.818134	35.689204
1331.674360	98259.878379	35.694221
1332.821420	98417.088650	35.699239
1334.419020	98565.706755	35.704256
1336.227014	98713.425672	35.709274
1337.319397	98864.498433	35.714292
1338.642931	99007.329973	35.719309
1340.298618	99158.340457	35.724327
1341.222204	99304.255181	35.729344
1342.730016	99449.938798	35.734362
1344.256473	99588.426955	35.739380
1345.547805	99735.019871	35.744397
1346.443942	99886.098929	35.749415
1347.939156	100045.403502	35.754432
1349.466854	100201.901229	35.759450
1350.755348	100346.075316	35.764468
1352.406232	100484.821161	35.769485
1353.654828	100639.398549	35.774503
1355.140401	100803.550025	35.779520
1356.334380	100937.018563	35.784538
1357.390199	101086.871651	35.789556
1358.991079	101231.628008	35.794573
1360.201280	101379.541339	35.799591
1361.608810	101532.175982	35.804608
1363.339681	101672.415798	35.809626
1364.597190	101834.073606	35.814644
1366.255145	101972.903188	35.819661
1367.484267	102118.856757	35.824679
1368.720135	102248.422209	35.829696
1370.099762	102381.629119	35.834714
1371.256303	102511.430102	35.839732
1372.639127	102642.929582	35.844749
1373.814285	102777.341836	35.849767
1375.198714	102910.165023	35.854784
1376.551177	103035.774243	35.859802
1377.669889	103200.715978	35.864820
1379.273080	103331.855279	35.869837
1380.910374	103475.069523	35.874855
1381.909732	103612.444250	35.879872
1383.432908	103753.552202	35.884890
1384.520950	103899.488688	35.889908
1386.117937	104048.205403	35.894925
1387.442741	104207.242858	35.899943
1388.352632	104358.386742	35.904960
1390.104258	104497.444234	35.909978
1391.278706	104664.741400	35.914996
1392.736927	104807.935266	35.920013
1394.297023	104967.547952	35.925031
1395.827391	105132.020146	35.930048
1397.319748	105281.729474	35.935066
1398.560580	105445.686645	35.940084
1400.146985	105597.104306	35.945101
1401.366606	105752.409859	35.950119
1402.879727	105899.221406	35.955136
1404.637558	106044.039494	35.960154
1405.966906	106218.157690	35.965172
1407.241640	106372.958587	35.970189
1408.401264	106520.899655	35.975207
1410.084847	106678.719567	35.980224
1411.766471	106839.540600	35.985242
1412.908251	107003.448285	35.990260
1414.246257	107152.212955	35.995277
1415.870309	107314.343711	36.000295
1417.567710	107477.989148	36.005312
1418.978992	107616.669620	36.010330
1420.483746	107782.676753	36.015348
1421.978458	107940.414736	36.020365
1423.506137	108087.832319	36.025383
1424.489689	108244.748476	36.030400
1426.209470	108397.561377	36.035418
1427.510582	108559.131590	36.040436
1429.037976	108716.989710	36.045453
1430.610442	108873.417638	36.050471
1432.230682	109030.516211	36.055488
1433.771212	109168.558476	36.060506
1434.852045	109338.491834	36.065524
1436.164932	109484.838108	36.070541
1437.596886	109638.318517	36.075559
1438.887240	109806.474950	36.080576
1440.589659	109962.382894	36.085594
1441.645915	110107.760978	36.090612
1443.532605	110267.363328	36.095629
1445.095612	110414.270419	36.100647
1446.136302	110568.439145	36.105664
1447.614800	110696.138377	36.110682
1448.794382	110844.761008	36.115700
1450.496589	110983.249930	36.120717
1451.691876	111132.878235	36.125735
1452.703242	111278.954017	36.130752
1454.285485	111434.649907	36.135770
1455.621573	111576.491852	36.140788
1456.842920	111739.323790	36.145805
1458.347208	111898.086007	36.150823
1459.848186	112060.033752	36.155840
1461.595883	112214.011844	36.160858
1462.598262	112377.547433	36.165876
1464.038155	112539.280140	36.170893
1465.807819	112704.632994	36.175911
1467.130335	112868.469116	36.180928
1468.412497	113032.806489	36.185946
1469.835798	113207.402885	36.190964
1471.556356	113371.147430	36.195981
1473.321335	113535.715272	36.200999
1474.620401	113714.778874	36.206016
1476.036127	113868.155277	36.211034
1477.912823	114038.747929	36.216052
1479.289904	114217.923022	36.221069
1481.036839	114383.999657	36.226087
1481.957553	114561.945616	36.231104
1483.885064	114719.449456	36.236122
1485.458907	114887.247209	36.241140
1486.881818	115063.977412	36.246157
1488.311754	115226.995262	36.251175
1489.848193	115413.168070	36.256192
1491.196054	115567.483610	36.261210
1493.066426	115739.342332	36.266228
1494.568221	115929.804150	36.271245
1496.237385	116082.786607	36.276263
1497.944416	116257.682025	36.281280
1499.668115	116409.834759	36.286298
1501.292768	116588.259293	36.291316
1502.337556	116757.400744	36.296333
1503.965166	116911.585059	36.301351
1505.519830	117079.115495	36.306368
1506.988187	117239.360771	36.311386
1508.712533	117414.255062	36.316404
1509.955243	117570.929410	36.321421
1511.753324	117740.673153	36.326439
1513.218628	117905.658986	36.331456
1514.733861	118067.472206	36.336474
1516.273132	118242.433215	36.341492
1517.698715	118406.998038	36.346509
1519.354579	118571.938888	36.351527
1520.797483	118742.518139	36.356544
1522.238171	118894.186101	36.361562
1523.987090	119051.992091	36.366580
1525.101655	119230.902302	36.371597
1526.863415	119392.228799	36.376615
1527.943949	119547.807554	36.381632
1529.662322	119692.566033	36.386650
1531.146897	119847.879787	36.391668
1532.280539	119994.892027	36.396685
1533.835827	120155.211299	36.401703
1535.293383	120319.954184	36.406720
1537.009136	120473.791251	36.411738
1538.417986	120633.731480	36.416756
1539.533902	120797.176579	36.421773
1541.093220	120955.866442	36.426791
1542.796217	121124.197434	36.431808
1544.274727	121282.750144	36.436826
1545.450076	121472.671597	36.441844
1547.213311	121643.972550	36.446861
1548.993855	121812.004353	36.451879
1550.032088	121992.338762	36.456896
1551.642047	122172.368284	36.461914
1553.326686	122342.723736	36.466932
1554.788310	122517.763818	36.471949
1556.557264	122704.142280	36.476967
1558.074838	122901.631474	36.481984
1559.663291	123079.720137	36.487002
1561.114972	123257.553082	36.492020
1562.372563	123443.296036	36.497037
1564.411972	123627.054250	36.502055
1566.151179	123819.689451	36.507072
1567.756986	124001.999237	36.512090
1569.516982	124176.217582	36.517108
1571.081195	124367.098637	36.522125
1572.800377	124549.330822	36.527143
1574.338769	124740.370634	36.532160
1576.150887	124918.157400	36.537178
1578.127469	125098.946483	36.542196
1579.522975	125280.449733	36.547213
1581.353451	125445.405966	36.552231
1582.544661	125631.681313	36.557248
1584.338197	125806.208917	36.562266
1585.815541	125971.629793	36.567284
1587.583564	126155.144448	36.572301
1589.135055	126332.817277	36.577319
1590.891588	126525.139790	36.582336
1592.515252	126687.704387	36.587354
1593.925218	126867.379265	36.592372
1595.090741	127046.296115	36.597389
1597.280656	127226.520854	36.602407
1598.828781	127409.483546	36.607424
1600.205901	127592.563296	36.612442
1602.376977	127753.755228	36.617460
1603.590464	127943.159113	36.622477
1605.285782	128117.007764	36.627495
1606.844161	128287.686969	36.632512
1608.560038	128470.731454	36.637530
1610.268463	128643.415908	36.642548
1612.201124	128816.597893	36.647565
1613.893148	128978.265817	36.652583
1614.997054	129137.431105	36.657600
1616.390304	129291.395356	36.662618
1618.147080	129454.195931	36.667636
1619.681123	129617.995642	36.672653
1621.213162	129760.070118	36.677671
1622.654992	129937.213647	36.682688
1624.360270	130099.468775	36.687706
1625.328623	130263.362135	36.692724
1627.060855	130432.557401	36.697741
1628.945014	130612.688171	36.702759
1630.206072	130788.066838	36.707776
1631.997037	130958.244147	36.712794
1633.392065	131147.615782	36.717812
1635.097331	131323.750757	36.722829
1636.760438	131508.014562	36.727847
1638.344948	131693.014213	36.732864
1639.923724	131878.674806	36.737882
1641.877159	132059.513369	36.742900
1643.260106	132256.825542	36.747917
1645.124259	132427.975698	36.752935
1646.776409	132612.311816	36.757952
1648.250604	132815.884956	36.762970
1649.937169	133005.172097	36.767988
1651.389788	133186.325460	36.773005
1653.648141	133374.700709	36.778023
1655.079158	133573.154724	36.783040
1656.745716	133760.042724	36.788058
1658.913091	133939.490916	36.793076
1660.473953	134133.480899	36.798093
1662.428302	134326.446749	36.803111
1664.045386	134503.515107	36.808128
1665.871012	134697.555562	36.813146
1667.379729	134877.076215	36.818164
1669.021373	135068.487519	36.823181
1670.974232	135237.258328	36.828199
1672.376764	135437.643090	36.833216
1674.243683	135617.048118	36.838234
1676.091443	135805.681947	36.843252
1677.680115	135988.871475	36.848269
1679.700553	136162.097255	36.853287
1681.295389	136349.659707	36.858304
1683.172993	136539.738120	36.863322
1684.735837	136713.838160	36.868340
1686.161623	136900.315903	36.873357
1687.800843	137087.103084	36.878375
1689.440010	137272.763672	36.883392
1691.550634	137449.150753	36.888410
1693.385212	137632.108815	36.893428
1694.378057	137826.720606	36.898445
1696.530882	138009.364372	36.903463
1698.212001	138188.688011	36.908480
1700.257406	138372.960469	36.913498
1702.058891	138551.063330	36.918516
1703.383907	138733.019321	36.923533
1705.472181	138890.916780	36.928551
1707.052955	139059.363250	36.933568
1708.343961	139227.197706	36.938586
1710.350563	139383.691420	36.943604
1711.802437	139540.400768	36.948621
1713.299342	139704.568127	36.953639
1715.161901	139870.427202	36.958656
1716.513970	140035.797969	36.963674
1718.094053	140206.747635	36.968692
1719.509686	140388.116401	36.973709
1721.423051	140562.107439	36.978727
1723.011860	140731.715353	36.983744
1724.619546	140922.371758	36.988762
1726.424153	141107.447117	36.993780
1727.597187	141299.277515	36.998797
1729.597583	141496.034558	37.003815
1731.042030	141676.747491	37.008832
1732.917440	141873.780314	37.013850
1734.891673	142072.471682	37.018868
1736.503831	142272.096345	37.023885
1738.255611	142461.801712	37.028903
1739.966694	142665.443602	37.033920
1741.687857	142863.153716	37.038938
1743.852894	143055.205271	37.043956
1745.401137	143260.664065	37.048973
1747.155527	143454.050762	37.053991
1749.307873	143666.716864	37.059008
1750.711377	143865.155637	37.064026
1752.630194	144057.049772	37.069044
1754.363478	144256.516063	37.074061
1756.287812	144453.785910	37.079079
1758.618820	144644.147976	37.084096
1760.533048	144840.078350	37.089114
1762.346210	145029.739152	37.094132
1764.173647	145231.313530	37.099149
1766.160932	145421.532143	37.104167
1768.124788	145600.766113	37.109184
1770.011365	145789.798809	37.114202
1771.591661	145963.949540	37.119220
1773.318030	146155.684415	37.124237
1775.166943	146339.237895	37.129255
1777.052795	146518.362761	37.134272
1778.725794	146710.413722	37.139290
1780.701509	146893.696802	37.144308
1782.468617	147084.087243	37.149325
1783.977052	147266.838231	37.154343
1786.099937	147453.130773	37.159360
1787.856244	147645.731958	37.164378
1789.512194	147806.748381	37.169396
1791.119546	147999.235924	37.174413
1793.027509	148192.386791	37.179431
1794.833274	148372.257448	37.184448
1796.637539	148558.784538	37.189466
1798.598303	148735.362096	37.194484
1800.052003	148936.804030	37.199501
1801.673002	149123.718461	37.204519
1804.091451	149287.131328	37.209536
1805.787339	149448.783552	37.214554
1807.053847	149605.674833	37.219572
1809.261893	149767.171299	37.224589
1810.864108	149936.180835	37.229607
1812.925588	150104.484498	37.234624
1814.138385	150273.354782	37.239642
1815.960273	150426.777087	37.244660
1817.575461	150616.604208	37.249677
1819.691830	150798.112565	37.254695
1821.403928	150974.627794	37.259712
1822.900934	151145.625358	37.264730
1824.580810	151335.649255	37.269748
1826.354529	151530.007812	37.274765
1828.281594	151715.519458	37.279783
1829.858880	151913.981044	37.284800
1831.535839	152101.740524	37.289818
1833.539433	152307.363239	37.294836
1835.649649	152511.639119	37.299853
1837.167517	152705.918480	37.304871
1839.192696	152899.459194	37.309888
1840.594571	153093.873354	37.314906
1842.561598	153314.151594	37.319924
1844.579850	153518.942762	37.324941
1846.325257	153728.697775	37.329959
1848.369477	153931.484156	37.334976
1849.866978	154139.480744	37.339994
1852.122310	154347.180840	37.345012
1854.082447	154552.722961	37.350029
1856.140205	154757.540830	37.355047
1858.458411	154956.448232	37.360064
1860.082724	155179.240235	37.365082
1862.123639	155372.475843	37.370100
1863.793900	155576.637496	37.375117
1866.070801	155775.011087	37.380135
1868.205843	155961.134713	37.385152
1869.379895	156170.919602	37.390170
1871.571493	156376.372717	37.395188
1873.797217	156575.507212	37.400205
1875.469195	156779.168650	37.405223
1877.938391	156971.521227	37.410240
1879.694351	157166.625493	37.415258
1881.644486	157357.553725	37.420276
1883.730734	157544.733508	37.425293
1885.637138	157736.190669	37.430311
1887.471122	157941.786039	37.435328
1889.318391	158127.295108	37.440346
1891.182293	158311.864197	37.445364
1893.325677	158513.318149	37.450381
1895.099192	158703.888791	37.455399
1897.185921	158882.605261	37.460416
1898.794465	159092.808220	37.465434
1900.643003	159274.164018	37.470452
1902.781768	159476.030072	37.475469
1904.649902	159645.794557	37.480487
1906.507679	159820.735278	37.485504
1908.067970	159990.575655	37.490522
1909.934173	160157.172714	37.495540
1911.728961	160323.325383	37.500557
1913.308448	160499.581754	37.505575
1915.310882	160673.552694	37.510592
1916.840477	160859.012587	37.515610
1918.991985	161034.534117	37.520628
1920.715068	161220.700714	37.525645
1922.251506	161403.347125	37.530663
1924.439950	161604.418588	37.535680
1926.196960	161799.548619	37.540698
1927.973224	161995.982866	37.545716
1930.064647	162195.120099	37.550733
1931.680307	162388.982256	37.555751
1934.072677	162590.064963	37.560768
1935.391663	162793.069230	37.565786
1937.877778	162994.481738	37.570804
1939.794737	163189.834922	37.575821
1941.626035	163400.091512	37.580839
1944.120939	163603.281521	37.585856
1946.010204	163812.161637	37.590874
1947.947906	164011.688423	37.595892
1949.929515	164221.773743	37.600909
1951.970344	164417.976299	37.605927
1953.916554	164627.118393	37.610944
1955.913087	164830.888971	37.615962
1958.091132	165023.128725	37.620980
1959.955000	165236.016063	37.625997
1961.798316	165438.457281	37.631015
1964.256749	165633.509369	37.636032
1966.068923	165826.686502	37.641050
1968.270968	166041.858495	37.646068
1970.636225	166242.813498	37.651085
1972.362950	166443.807495	37.656103
1974.298833	166633.658915	37.661120
1976.509834	166841.693493	37.666138
1978.278953	167036.989184	37.671156
1980.751545	167224.741807	37.676173
1982.652980	167433.424924	37.681191
1984.789461	167619.114721	37.686208
1986.728870	167820.691194	37.691226
1988.631465	168021.538937	37.696244
1990.537538	168214.053991	37.701261
1992.665527	168399.761673	37.706279
1994.398553	168609.695676	37.711296
1996.248292	168817.468740	37.716314
1998.383709	169010.090978	37.721332
2000.445903	169211.782227	37.726349
2002.723546	169405.309837	37.731367
2005.076389	169599.942707	37.736384
2007.187905	169799.168505	37.741402
2009.071453	169975.891482	37.746420
2011.145942	170162.948110	37.751437
2013.027137	170342.704715	37.756455
2015.111042	170521.808458	37.761472
2016.950092	170694.647661	37.766490
2018.921000	170856.710175	37.771508
2020.940504	171011.700309	37.776525
2022.645356	171182.863243	37.781543
2024.521232	171347.936483	37.786560
2026.513801	171520.247624	37.791578
2028.291222	171700.306066	37.796596
2029.894661	171886.646613	37.801613
2031.998484	172074.532342	37.806631
2034.019827	172256.267122	37.811648
2036.135525	172451.751125	37.816666
2038.408878	172642.175074	37.821684
2040.406111	172838.212571	37.826701
2042.286914	173039.736880	37.831719
2044.853552	173226.755519	37.836736
2046.841546	173423.266745	37.841754
2048.694796	173619.432441	37.846772
2050.868782	173797.851879	37.851789
2052.658956	174006.359844	37.856807
2054.742068	174198.838472	37.861824
2057.135565	174401.100234	37.866842
2059.181684	174588.804085	37.871860
2060.976546	174791.632161	37.876877
2062.829943	175000.325557	37.881895
2065.491564	175188.315144	37.886912
2067.512730	175389.778303	37.891930
2069.488721	175598.176249	37.896948
2072.245253	175790.568352	37.901965
2074.130263	175981.463098	37.906983
2076.412657	176168.540558	37.912000
2078.361676	176376.972150	37.917018
2080.574288	176573.501189	37.922036
2082.741497	176765.496615	37.927053
2084.639757	176962.052011	37.932071
2086.753265	177148.450300	37.937088
2088.837821	177340.207793	37.942106
2090.904788	177546.850483	37.947124
2093.388788	177744.864479	37.952141
2095.495989	177937.306238	37.957159
2097.758120	178121.452459	37.962176
2099.897359	178326.412904	37.967194
2102.024520	178510.544197	37.972212
2104.430498	178704.566050	37.977229
2106.532303	178891.773317	37.982247
2108.484601	179075.414664	37.987264
2110.749870	179252.041879	37.992282
2113.050203	179445.893614	37.997300
2115.234190	179631.961977	38.002317
2117.147182	179810.664701	38.007335
2119.332431	180003.636448	38.012352
2121.487174	180180.056707	38.017370
2123.777288	180375.373389	38.022388
2126.170323	180545.451648	38.027405
2127.750032	180719.250202	38.032423
2129.945992	180873.247688	38.037440
2132.084247	181025.148714	38.042458
2133.888327	181198.786751	38.047476
2135.962944	181353.883678	38.052493
2137.691700	181525.390735	38.057511
2139.540427	181678.786419	38.062528
2141.706541	181857.774763	38.067546
2143.401530	182029.542939	38.072564
2145.965542	182201.808370	38.077581
2147.709569	182393.312909	38.082599
2149.842625	182567.221475	38.087616
2151.833389	182762.647229	38.092634
2153.736345	182948.673046	38.097652
2156.298140	183145.139205	38.102669
2158.039832	183347.243096	38.107687
2160.455862	183545.662811	38.112704
2162.424946	183728.141355	38.117722
2164.549556	183944.461875	38.122740
2166.785885	184147.138104	38.127757
2168.920561	184351.430161	38.132775
2171.555842	184555.872162	38.137792
2173.908636	184753.406419	38.142810
2176.159643	184954.003030	38.147828
2178.299696	185158.475580	38.152845
2180.505254	185367.062604	38.157863
2182.780402	185553.662091	38.162880
2185.138114	185757.747558	38.167898
2187.360867	185967.844645	38.172916
2189.886667	186166.956525	38.177933
2191.801818	186353.413383	38.182951
2193.959097	186554.590315	38.187968
2196.520406	186766.071306	38.192986
2198.432929	186974.712211	38.198004
2200.795052	187170.682075	38.203021
2202.770291	187380.253906	38.208039
2205.437217	187570.784075	38.213056
2207.677738	187765.075352	38.218074
2209.576820	187977.529845	38.223092
2212.037687	188181.064128	38.228109
2214.384976	188386.190858	38.233127
2216.210869	188579.586876	38.238144
2218.562742	188791.579904	38.243162
2221.164107	188992.290979	38.248180
2223.625698	189199.420875	38.253197
2225.542598	189397.691522	38.258215
2228.115642	189593.587417	38.263232
2229.957208	189795.907163	38.268250
2232.023744	190004.181916	38.273268
2234.468771	190196.877283	38.278285
2236.660433	190402.456283	38.283303
2238.307274	190615.470333	38.288320
2240.918703	190818.344953	38.293338
2242.943171	191031.478644	38.298356
2245.567117	191227.982358	38.303373
2247.652751	191439.458383	38.308391
2250.101179	191610.013706	38.313408
2252.301697	191780.164766	38.318426
2254.246880	191962.387791	38.323444
2256.541192	192137.487341	38.328461
2258.537550	192321.975265	38.333479
2260.605977	192505.043767	38.338496
2262.752000	192700.740881	38.343514
2264.820109	192903.075859	38.348532
2267.034692	193094.017224	38.353549
2269.073120	193294.099505	38.358567
2271.097687	193502.776739	38.363584
2273.334823	193698.945649	38.368602
2275.290207	193929.718434	38.373620
2277.551602	194144.046527	38.378637
2279.968976	194360.013387	38.383655
2282.032718	194585.581241	38.388672
2284.787788	194796.990975	38.393690
2286.630875	195041.848921	38.398708
2289.124872	195260.320448	38.403725
2291.126479	195486.206794	38.408743
2293.937161	195707.701439	38.413760
2296.666102	195936.038208	38.418778
2298.537608	196176.721527	38.423796
2301.318491	196386.928089	38.428813
2303.397196	196625.232661	38.433831
2305.349610	196852.490900	38.438848
2308.153356	197089.324624	38.443866
2310.452892	197327.102440	38.448884
2312.683222	197542.719024	38.453901
2315.197545	197790.961372	38.458919
2317.549714	198020.826734	38.463936
2319.788093	198247.487282	38.468954
2322.226262	198489.843066	38.473972
2324.831001	198719.747606	38.478989
2327.241777	198953.288583	38.484007
2329.358927	199183.208978	38.489024
2331.956888	199416.125768	38.494042
2334.315508	199656.620994	38.499060
2336.538564	199882.643649	38.504077
2338.656002	200121.084891	38.509095
2341.034578	200354.586339	38.514112
2343.881079	200581.401602	38.519130
2345.841625	200819.718490	38.524148
2348.605311	201056.271703	38.529165
2350.854018	201300.510751	38.534183
2353.164698	201526.310603	38.539200
2355.725037	201756.514432	38.544218
2357.886332	202001.900160	38.549236
2360.301015	202224.233827	38.554253
2362.696237	202474.877687	38.559271
2365.014501	202715.684779	38.564288
2367.661706	202931.168053	38.569306
2369.935620	203182.595939	38.574324
2372.338240	203414.202556	38.579341
2374.804752	203633.207913	38.584359
2376.972158	203845.521189	38.589376
2379.281389	204040.574700	38.594394
2381.399015	204247.400992	38.599412
2383.377257	204463.529313	38.604429
2385.552954	204679.081317	38.609447
2387.809787	204894.545109	38.614464
2390.252609	205124.337103	38.619482
2392.046739	205350.983171	38.624500
2394.431417	205580.481543	38.629517
2396.633873	205824.341367	38.634535
2398.991168	206058.682430	38.639552
2401.700709	206301.702227	38.644570
2403.651092	206554.909924	38.649588
2406.538406	206806.751548	38.654605
2408.704037	207056.855257	38.659623
2410.977060	207290.173651	38.664640
2413.435425	207554.438133	38.669658
2415.508610	207827.587547	38.674676
2417.983728	208083.435228	38.679693
2420.319822	208348.001874	38.684711
2422.676521	208625.680052	38.689728
2425.376229	208887.474757	38.694746
2428.052036	209158.135366	38.699764
2430.334240	209426.701429	38.704781
2433.309013	209691.591623	38.709799
2435.653718	209956.633599	38.714816
2438.259671	210222.473179	38.719834
2440.423909	210491.722716	38.724852
2443.199190	210765.535693	38.729869
2445.997198	211026.206726	38.734887
2448.431275	211307.096596	38.739904
2450.911787	211563.846557	38.744922
2453.212965	211829.855512	38.749940
2455.593531	212098.493645	38.754957
2458.315795	212363.333589	38.759975
2460.946877	212639.196099	38.764992
2463.461879	212900.186271	38.770010
2465.982524	213166.419897	38.775028
2468.652644	213437.633024	38.780045
2471.498198	213699.450024	38.785063
2473.624313	213966.206483	38.790080
2476.136973	214222.390611	38.795098
2478.724225	214484.759504	38.800116
2481.342688	214749.816026	38.805133
2484.159647	215014.842147	38.810151
2486.641286	215274.678993	38.815168
2489.229189	215530.145247	38.820186
2491.673252	215792.795880	38.825204
2494.265475	216048.733164	38.830221
2496.324348	216296.312939	38.835239
2498.684289	216569.352713	38.840256
2501.226557	216818.851086	38.845274
2503.660422	217097.302568	38.850292
2505.843398	217359.200700	38.855309
2508.671878	217605.088856	38.860327
2510.760860	217872.285537	38.865344
2513.670109	218095.778669	38.870362
2515.839867	218339.285255	38.875380
2518.100320	218574.576276	38.880397
2520.455612	218812.849465	38.885415
2522.523426	219069.363409	38.890432
2525.383474	219311.024480	38.895450
2527.455637	219576.046376	38.900468
2529.586437	219825.277753	38.905485
2532.285897	220096.474398	38.910503
2534.717513	220369.250822	38.915520
2537.478536	220629.075913	38.920538
2539.904127	220913.003271	38.925556
2542.094472	221189.642766	38.930573
2544.941954	221465.976009	38.935591
2547.409301	221748.008055	38.940608
2549.792623	222046.345023	38.945626
2552.332886	222373.430355	38.950644
2554.650418	222650.524854	38.955661
2557.614422	222938.577346	38.960679
2559.841042	223243.102044	38.965696
2562.875617	223531.755044	38.970714
2565.354594	223827.277625	38.975732
2567.995581	224124.553311	38.980749
2570.637872	224419.937966	38.985767
2573.288339	224711.754380	38.990784
2576.079263	225007.422413	38.995802
2578.515305	225315.959807	39.000820
2581.334063	225607.079834	39.005837
2584.337105	225899.962107	39.010855
2586.633673	226205.337816	39.015872
2589.378107	226492.612614	39.020890
2591.889998	226793.359731	39.025908
2594.449976	227093.109869	39.030925
2597.438464	227382.914084	39.035943
2599.942420	227682.192676	39.040960
2602.873604	227982.852233	39.045978
2605.310989	228283.895839	39.050996
2608.193250	228577.708202	39.056013
2611.130547	228858.154234	39.061031
2613.352629	229166.625440	39.066048
2616.128890	229453.371884	39.071066
2618.823914	229751.535324	39.076084
2621.652248	230050.719925	39.081101
2624.335032	230337.636427	39.086119
2626.924405	230637.546569	39.091136
2629.662284	230932.938879	39.096154
2631.994029	231219.989989	39.101172
2634.658487	231516.894262	39.106189
2637.490669	231806.407667	39.111207
2639.889908	232096.320729	39.116224
2642.621081	232395.426834	39.121242
2645.615277	232677.653569	39.126260
2648.251892	232974.084338	39.131277
2650.909758	233248.391159	39.136295
2653.238855	233526.306550	39.141312
2655.486751	233778.685251	39.146330
2658.209405	234040.615259	39.151348
2660.300433	234310.341646	39.156365
2662.921445	234581.534111	39.161383
2665.233146	234864.281718	39.166400
2667.790115	235139.600369	39.171418
2670.220982	235422.432273	39.176436
2672.562575	235725.674070	39.181453
2675.027334	236019.753789	39.186471
2677.375814	236333.308102	39.191488
2680.045205	236632.919456	39.196506
2682.586910	236951.804154	39.201524
2685.477905	237271.244067	39.206541
2688.706232	237575.036585	39.211559
2690.746526	237899.286530	39.216576
2693.580822	238219.957417	39.221594
2696.424438	238547.841129	39.226612
2699.223631	238874.412101	39.231629
2702.278058	239196.066951	39.236647
2705.026561	239522.165273	39.241664
2707.700386	239846.549208	39.246682
2710.293310	240179.887509	39.251700
2713.152032	240513.565675	39.256717
2716.109136	240830.109861	39.261735
2718.607426	241172.762284	39.266752
2721.784429	241496.842560	39.271770
2724.799031	241822.168636	39.276788
2727.562453	242151.396164	39.281805
2730.271765	242473.343357	39.286823
2733.062008	242803.355799	39.291840
2735.960950	243130.608694	39.296858
2738.646413	243467.091127	39.301876
2741.549019	243785.861485	39.306893
2744.484542	244112.349127	39.311911
2747.459796	244440.609333	39.316928
2750.128154	244763.381673	39.321946
2753.046934	245084.286309	39.326964
2755.889652	245406.168989	39.331981
2758.542786	245722.900736	39.336999
2761.245837	246073.459041	39.342016
2764.287191	246384.034676	39.347034
2766.988873	246701.853229	39.352052
2769.443839	247041.048303	39.357069
2772.304971	247356.836412	39.362087
2775.421345	247692.905586	39.367104
2778.327869	248020.753430	39.372122
2780.917739	248339.660162	39.377140
2783.603731	248666.782330	39.382157
2786.499139	249000.501763	39.387175
2789.087979	249324.973612	39.392192
2792.124131	249654.430172	39.397210
2795.046537	249980.044433	39.402228
2797.564606	250312.607177	39.407245
2800.234876	250624.698325	39.412263
2802.748518	250915.985632	39.417280
2805.216869	251216.577599	39.422298
2808.112175	251525.561239	39.427316
2810.660758	251826.039993	39.432333
2813.336992	252135.135642	39.437351
2815.677357	252455.512598	39.442368
2818.623696	252767.564010	39.447386
2821.349126	253084.909131	39.452404
2823.316380	253421.832703	39.457421
2826.538219	253745.679468	39.462439
2829.237691	254080.100526	39.467456
2831.922371	254428.267013	39.472474
2834.734590	254767.751836	39.477492
2837.358418	255120.120548	39.482509
2840.485159	255461.639748	39.487527
2843.022948	255828.858194	39.492544
2846.030574	256174.080774	39.497562
2848.871653	256536.603848	39.502580
2851.399761	256916.247459	39.507597
2854.536926	257265.007630	39.512615
2857.607359	257629.934853	39.517632
2860.585004	258003.590399	39.522650
2863.532360	258361.323987	39.527668
2866.443837	258733.492439	39.532685
2869.423487	259100.671773	39.537703
2872.480265	259471.192590	39.542720
2875.501108	259835.597609	39.547738
2878.626369	260203.288964	39.552756
2881.344489	260575.566976	39.557773
2884.542837	260934.077394	39.562791
2887.561965	261310.271586	39.567808
2890.434743	261674.346905	39.572826
2893.418896	262043.688841	39.577844
2896.020825	262416.698955	39.582861
2899.230762	262786.361698	39.587879
2902.108809	263167.254709	39.592896
2905.082329	263531.849753	39.597914
2908.271648	263901.186796	39.602932
2910.987717	264281.293826	39.607949
2914.084464	264644.702004	39.612967
2916.976110	265012.385324	39.617984
2919.825153	265386.528130	39.623002
2922.848853	265765.825879	39.628020
2925.841707	266135.653493	39.633037
2928.808569	266499.287173	39.638055
2931.617482	266885.199344	39.643072
2934.445491	267259.169310	39.648090
2937.623498	267624.853521	39.653108
2940.030789	268020.051548	39.658125
2943.143023	268396.111241	39.663143
2946.355831	268773.857290	39.668160
2949.233539	269150.005413	39.673178
2952.481187	269530.896431	39.678196
2955.309895	269913.276572	39.683213
2958.201469	270272.479132	39.688231
2961.055683	270620.789747	39.693248
2963.858841	270962.681547	39.698266
2966.828951	271300.203084	39.703284
2969.246853	271645.128323	39.708301
2972.182013	271990.098826	39.713319
2975.519658	272330.661754	39.718336
2977.925036	272682.295800	39.723354
2980.695110	273041.696461	39.728372
2983.337507	273408.713035	39.733389
2986.515615	273774.831987	39.738407
2989.558569	274148.644228	39.743424
2991.892538	274525.617148	39.748442
2995.164643	274899.266200	39.753460
2997.918174	275294.945915	39.758477
3000.955627	275688.777066	39.763495
3004.191402	276079.630035	39.768512
3006.837125	276476.165132	39.773530
3010.191652	276878.913470	39.778548
3012.835015	277277.963805	39.783565
3016.075383	277678.596220	39.788583
3018.965311	278080.579595	39.793600
3021.866396	278490.182131	39.798618
3025.127536	278895.383591	39.803636
3027.796211	279319.807434	39.808653
3030.791571	279744.687485	39.813671
3034.421199	280158.670553	39.818688
3037.340297	280586.610707	39.823706
3040.461247	281005.043256	39.828724
3043.426376	281436.100285	39.833741
3046.768183	281852.693771	39.838759
3049.886282	282273.920395	39.843776
3052.889761	282696.689070	39.848794
3056.505326	283122.281952	39.853812
3059.538048	283547.331660	39.858829
3062.527239	283962.658483	39.863847
3065.803094	284377.837982	39.868864
3069.062329	284807.677372	39.873882
3072.035495	285235.097515	39.878900
3075.268367	285660.647113	39.883917
3078.270912	286080.110574	39.888935
3081.411611	286498.967458	39.893952
3084.518121	286926.517125	39.898970
3087.957813	287340.524578	39.903988
3091.121390	287767.683166	39.909005
3094.167433	288185.714759	39.914023
3097.439835	288606.732945	39.919040
3100.420129	289031.886656	39.924058
3103.734302	289444.996812	39.929076
3106.838350	289870.841040	39.934093
3110.049460	290283.712295	39.939111
3113.200255	290694.103019	39.944128
3115.887737	291121.713243	39.949146
3119.273903	291542.277307	39.954164
3122.282748	291968.819193	39.959181
3125.493299	292367.461841	39.964199
3128.371785	292757.367113	39.969216
3131.247759	293146.789501	39.974234
3134.407358	293526.462639	39.979252
3137.096655	293933.212295	39.984269
3140.007275	294315.565354	39.989287
3142.912602	294707.292031	39.994304
3145.743545	295116.557312	39.999322
3148.754201	295527.520714	40.004340
3151.707021	295940.981856	40.009357
3154.740923	296359.560546	40.014375
3158.094501	296774.023449	40.019392
3160.869100	297210.880003	40.024410
3164.016196	297633.172125	40.029428
3167.026549	298070.954656	40.034445
3170.045157	298500.098220	40.039463
3173.516947	298956.094901	40.044480
3176.496952	299406.351219	40.049498
3179.670691	299855.940671	40.054516
3183.000854	300310.635290	40.059533
3185.800098	300776.817911	40.064551
3189.339097	301223.170693	40.069568
3192.353295	301689.900903	40.074586
3196.106307	302159.611801	40.079604
3199.115445	302623.596680	40.084621
3202.261527	303095.890030	40.089639
3205.990666	303565.219336	40.094656
3209.149900	304031.639985	40.099674
3212.532888	304489.616053	40.104692
3215.879061	304965.885007	40.109709
3218.988983	305441.554691	40.114727
3222.708579	305897.237634	40.119744
3225.894996	306369.513701	40.124762
3229.401550	306834.726943	40.129780
3232.793338	307307.779982	40.134797
3236.081423	307761.238728	40.139815
3239.482774	308225.091994	40.144832
3242.414080	308690.668899	40.149850
3245.636036	309163.792657	40.154868
3249.096112	309628.748969	40.159885
3252.269727	310107.007455	40.164903
3255.674672	310576.108957	40.169920
3258.821497	311045.655798	40.174938
3262.271749	311510.987232	40.179956
3265.612782	311987.001755	40.184973
3268.786549	312455.624151	40.189991
3272.722111	312922.523935	40.195008
3275.539323	313396.532541	40.200026
3279.130145	313862.238275	40.205044
3282.503988	314328.738262	40.210061
3285.719471	314788.124213	40.215079
3289.176512	315253.057619	40.220096
3292.270150	315720.383060	40.225114
3295.089411	316193.210391	40.230132
3298.798583	316662.389808	40.235149
3301.691942	317114.780924	40.240167
3304.707615	317543.835290	40.245184
3307.576132	317995.794503	40.250202
3311.015685	318426.631969	40.255220
3314.134676	318856.984839	40.260237
3317.222951	319310.147561	40.265255
3320.410123	319754.149393	40.270272
3323.679941	320206.720298	40.275290
3326.676722	320660.170253	40.280308
3329.796802	321127.109643	40.285325
3333.283650	321582.585414	40.290343
3337.176206	322036.674063	40.295360
3339.986654	322514.347157	40.300378
3343.229035	322979.124118	40.305396
3346.637888	323458.551320	40.310413
3349.492235	323939.079366	40.315431
3353.239369	324421.545975	40.320448
3356.209090	324908.272267	40.325466
3359.553169	325411.672286	40.330484
3363.271738	325913.384681	40.335501
3366.464745	326408.675860	40.340519
3370.011312	326918.942070	40.345536
3373.330876	327419.235242	40.350554
3376.904306	327925.503695	40.355572
3380.433092	328430.506188	40.360589
3383.546662	328941.970475	40.365607
3387.098110	329456.866540	40.370624
3390.406176	329974.006893	40.375642
3393.898434	330492.231902	40.380660
3397.774342	331014.506451	40.385677
3401.045673	331534.358917	40.390695
3404.795354	332038.489635	40.395712
3408.095882	332558.964997	40.400730
3411.455609	333069.625461	40.405748
3415.192008	333589.948212	40.410765
3418.580326	334115.349927	40.415783
3421.951079	334636.103620	40.420800
3425.350821	335164.568101	40.425818
3429.363175	335673.735140	40.430836
3433.022674	336184.503067	40.435853
3436.087283	336713.719469	40.440871
3440.020991	337213.797036	40.445888
3443.464942	337738.197082	40.450906
3446.445141	338257.511843	40.455924
3450.430522	338776.511203	40.460941
3453.690516	339297.398434	40.465959
3457.678252	339808.771852	40.470976
3460.923124	340325.844491	40.475994
3464.584824	340832.767083	40.481012
3467.830927	341346.987421	40.486029
3471.193097	341867.659547	40.491047
3475.009357	342372.666289	40.496064
3478.137507	342895.753309	40.501082
3481.680440	343413.743197	40.506100
3485.313081	343929.784889	40.511117
3488.868412	344435.195764	40.516122
3492.166974	344887.925491	40.521127
3494.884683	345300.527417	40.526132
3497.795586	345668.069374	40.531136
3500.606617	345986.704225	40.536141
3502.544607	346255.511419	40.541146
3504.866201	346481.776107	40.546151
3506.570250	346665.402518	40.551156
3508.136976	346808.911312	40.556160
3509.814110	346913.052659	40.561165
3511.190465	346992.883308	40.566170
3512.115646	347040.638669	40.571175
3513.281379	347065.397828	40.576180
3513.938543	347052.414977	40.581184
3514.587207	347019.555063	40.586189
3515.239296	346982.138588	40.591194
3515.570219	346907.790304	40.596199
3515.730229	346837.872238	40.601204
3516.111530	346749.567766	40.606208
3516.294783	346640.652349	40.611213
3516.120355	346535.636627	40.616218
3516.277539	346422.117975	40.621223
3516.094230	346299.057209	40.626228
3516.257467	346175.737777	40.631232
3516.164315	346047.749818	40.636237
3515.884506	345912.766056	40.641242
3515.918091	345777.350645	40.646247
3515.487492	345660.410892	40.651252
3514.962247	345518.032704	40.656256
3514.812718	345383.485278	40.661261
3514.544694	345268.453487	40.666266
3514.461157	345138.502110	40.671271
3514.215917	345019.190068	40.676276
3513.978794	344890.102381	40.681280
3513.687572	344759.190311	40.686285
3513.170921	344657.356083	40.691290
3513.260133	344534.681232	40.696295
3513.128193	344415.070070	40.701300
3512.479448	344309.259901	40.706304
3512.297932	344198.615838	40.711309
3512.447892	344093.519003	40.716314
3512.192423	343980.264485	40.721319
3511.830256	343878.735402	40.726324
3511.501046	343778.931802	40.731328
3511.580056	343679.903487	40.736333
3511.223688	343584.711024	40.741338
3511.135908	343491.435913	40.746343
3510.768113	343399.070359	40.751348
3510.559522	343301.105046	40.756352
3510.020138	343218.617083	40.761357
3509.779009	343134.045526	40.766362
3509.817956	343056.658575	40.771367
3509.597745	342983.232448	40.776372
3509.418404	342917.181513	40.781376
3509.330572	342832.178032	40.786381
3508.696263	342775.718776	40.791386
3508.733123	342702.124400	40.796391
3508.495475	342652.602277	40.801396
3508.418771	342587.909297	40.806400
3508.244200	342530.384416	40.811405
3508.149854	342484.861306	40.816410
3508.230196	342420.983320	40.821415
3507.846593	342371.484042	40.826420
3508.046085	342321.739822	40.831424
3507.866533	342262.942751	40.836429
3507.781891	342214.057905	40.841434
3507.712126	342176.650688	40.846439
3507.586368	342115.095876	40.851444
3507.324197	342066.824432	40.856448
3507.138308	342020.780900	40.861453
3507.202629	341987.476026	40.866458
3507.111419	341933.424697	40.871463
3507.054063	341903.677214	40.876468
3506.795017	341868.310652	40.881472
3506.978455	341813.910346	40.886477
3506.729054	341796.691444	40.891482
3506.677586	341759.281081	40.896487
3506.696713	341728.935964	40.901492
3506.791814	341694.353328	40.906496
3506.690388	341658.299905	40.911501
3506.369684	341635.721266	40.916506
3506.406481	341596.871383	40.921511
3506.289919	341566.114903	40.926516
3505.905860	341533.695218	40.931520
3506.307775	341503.569483	40.936525
3506.106724	341484.281007	40.941530
3506.075461	341447.758182	40.946535
3506.140550	341429.038536	40.951540
3506.285343	341407.989888	40.956544
3506.115997	341370.903383	40.961549
3505.647270	341354.635406	40.966554
3506.155686	341326.936423	40.971559
3506.059940	341304.958477	40.976564
3506.093800	341277.487218	40.981568
3506.024907	341251.992223	40.986573
3505.770560	341225.890160	40.991578
3505.750045	341196.391063	40.996583
3505.700236	341184.816903	41.001588
3505.960548	341160.720765	41.006592
3505.992775	341128.795073	41.011597
3505.672502	341116.907285	41.016602
3505.625197	341088.939673	41.021607
3505.527700	341067.725571	41.026612
3505.513476	341052.632965	41.031616
3505.981317	341023.412958	41.036621
3505.844669	341009.230622	41.041626
3505.783555	340979.508744	41.046631
3505.511194	340966.213324	41.051636
3505.357301	340936.582457	41.056640
3505.579999	340918.448665	41.061645
3505.163139	340896.674066	41.066650
3505.417308	340878.102551	41.071655
3505.167074	340871.600129	41.076660
3505.002147	340860.578665	41.081664
3505.184909	340844.996677	41.086669
3505.385459	340828.291848	41.091674
3505.502487	340812.771153	41.096679
3505.394246	340804.057136	41.101684
3505.396063	340777.888936	41.106688
3505.363309	340753.075314	41.111693
3505.137298	340743.259878	41.116698
3505.106080	340727.457135	41.121703
3505.529686	340709.189703	41.126708
3505.263689	340702.002465	41.131712
3505.316324	340680.102664	41.136717
3505.214148	340662.198339	41.141722
3505.199156	340645.120250	41.146727
3505.073816	340633.965212	41.151732
3504.919495	340616.323669	41.156736
3505.470279	340582.381129	41.161741
3505.034014	340577.409943	41.166746
3505.051178	340572.087073	41.171751
3505.229354	340543.294462	41.176756
3505.174749	340535.208310	41.181760
3505.375147	340521.252591	41.186765
3505.274009	340504.926284	41.191770
3505.038414	340490.734016	41.196775
3504.831258	340481.959225	41.201780
3504.845360	340471.825781	41.206784
3504.671564	340446.525228	41.211789
3504.649346	340450.474300	41.216794
3504.784002	340437.852631	41.221799
3504.983312	340427.435350	41.226804
3504.988548	340417.506941	41.231808
3504.775214	340404.863909	41.236813
3504.692716	340399.353136	41.241818
3505.040381	340380.232132	41.246823
3504.649715	340366.649821	41.251828
3504.755352	340353.269062	41.256832
3504.982135	340343.432897	41.261837
3504.719016	340338.816152	41.266842
3504.834541	340321.793710	41.271847
3504.808447	340308.306488	41.276852
3504.617021	340307.827630	41.281856
3504.983928	340284.121592	41.286861
3504.866815	340291.369416	41.291866
3504.845691	340263.422754	41.296871
3504.756451	340263.716858	41.301876
3504.709643	340241.298061	41.306880
3504.854392	340234.173117	41.311885
3504.728927	340221.948899	41.316890
3504.948691	340204.477205	41.321895
3504.761731	340192.822722	41.326900
3504.676423	340179.599387	41.331904
3504.852442	340172.342216	41.336909
3504.723469	340167.322422	41.341914
3504.854648	340149.890172	41.346919
3504.481565	340143.687104	41.351924
3504.525315	340139.658221	41.356928
3505.184601	340117.076851	41.361933
3504.765440	340118.950435	41.366938
3504.608767	340107.392970	41.371943
3504.670721	340107.281343	41.376948
3504.472857	340099.548702	41.381952
3504.711077	340088.132453	41.386957
3504.534692	340086.913008	41.391962
3504.800550	340063.859247	41.396967
3504.804390	340063.604074	41.401972
3504.539025	340054.202038	41.406976
3504.629491	340036.088896	41.411981
3504.540646	340039.564872	41.416986
3504.818063	340011.596360	41.421991
3504.746364	340010.513098	41.426996
3504.672199	339997.415241	41.432000
3504.844980	339984.354711	41.437005
3504.713605	339975.415137	41.442010
3504.541228	339959.303595	41.447015
3504.806488	339958.574354	41.452020
3504.580139	339944.864156	41.457024
3504.890378	339945.909689	41.462029
3504.502809	339939.607069	41.467034
3504.518235	339918.018351	41.472039
3504.718224	339910.350073	41.477044
3504.609333	339894.432122	41.482048
3504.784343	339891.222506	41.487053
3504.501384	339883.910579	41.492058
3504.404094	339859.234085	41.497063
3504.752328	339861.928223	41.502068
3504.346056	339846.795481	41.507072
3504.823341	339842.316213	41.512077
3504.770416	339831.684151	41.517082
3504.719500	339821.789982	41.522087
3504.755213	339803.481784	41.527092
3504.668011	339795.018857	41.532096
3504.381553	339786.078316	41.537101
3504.177608	339774.961007	41.542106
3504.469916	339768.525440	41.547111
3504.717035	339774.493879	41.552116
3504.480110	339757.908834	41.557120
3504.642268	339751.493839	41.562125
3504.335237	339747.265826	41.567130
3504.583415	339741.549990	41.572135
3504.308646	339728.127410	41.577140
3504.143523	339721.815061	41.582144
3504.645593	339706.869618	41.587149
3504.073170	339712.916703	41.592154
3504.216582	339709.075683	41.597159
3504.073032	339695.275976	41.602164
3504.022002	339692.483916	41.607168
3504.429100	339692.292273	41.612173
3504.144734	339691.522635	41.617178
3504.422615	339678.598162	41.622183
3504.311526	339680.499426	41.627188
3504.049745	339677.638858	41.632192
3504.616546	339672.967239	41.637197
3504.237957	339669.437834	41.642202
3504.806020	339655.296527	41.647207
3504.678055	339658.829619	41.652212
3504.369077	339634.873803	41.657216
3504.593906	339626.106972	41.662221
3504.473287	339620.398512	41.667226
3504.472320	339605.379831	41.672231
3504.440648	339605.384827	41.677236
3504.297693	339596.981598	41.682240
3504.558863	339575.990309	41.687245
3504.406767	339586.476610	41.692250
3504.659082	339578.901843	41.697255
3504.608287	339570.713144	41.702260
3504.135779	339569.005931	41.707264
3504.537014	339552.498141	41.712269
3504.590708	339536.554400	41.717274
3504.348007	339533.130785	41.722279
3504.491533	339529.747938	41.727284
3504.762992	339522.144682	41.732288
3504.746341	339506.950268	41.737293
3504.385969	339492.828412	41.742298
3504.410148	339483.176875	41.747303
3504.516359	339480.894519	41.752308
3504.461070	339475.735744	41.757312
3504.459976	339462.168023	41.762317
3504.446676	339460.795507	41.767322
3504.599427	339440.915907	41.772327
3504.363829	339429.879908	41.777332
3504.251771	339422.540912	41.782336
3504.370608	339414.987226	41.787341
3504.183640	339417.205962	41.792346
3504.163712	339412.016136	41.797351
3504.347564	339392.258882	41.802356
3504.108750	339387.358213	41.807360
3504.090422	339381.633561	41.812365
3504.222800	339388.842049	41.817370
3504.457276	339382.466498	41.822375
3504.733817	339373.462356	41.827380
3504.367173	339371.992960	41.832384
3505.005249	339354.454908	41.837389
3504.321640	339355.097531	41.842394
3504.579612	339344.619888	41.847399
3504.668456	339330.223339	41.852404
3504.330425	339320.679947	41.857408
3504.575915	339306.436821	41.862413
3504.403210	339302.162088	41.867418
3504.730376	339293.939061	41.872423
3504.480330	339287.156433	41.877428
3504.165455	339272.136385	41.882432
3504.510223	339268.110774	41.887437
3504.274122	339257.838498	41.892442
3504.562142	339238.370200	41.897447
3504.785408	339237.011195	41.902452
3504.539230	339223.736724	41.907456
3504.593885	339213.265744	41.912461
3504.505138	339202.104669	41.917466
3504.778551	339185.871550	41.922471
3504.577359	339195.780193	41.927476
3504.208748	339177.764833	41.932480
3504.409905	339162.026790	41.937485
3504.294490	339164.183312	41.942490
3504.184079	339154.349355	41.947495
3504.054058	339142.100194	41.952500
3504.050725	339137.595030	41.957504
3504.344056	339134.646686	41.962509
3504.202009	339137.469270	41.967514
3504.260062	339118.699140	41.972519
3504.401202	339108.850867	41.977524
3504.225351	339115.013509	41.982528
3504.646839	339106.877372	41.987533
3504.497551	339092.951162	41.992538
3504.527059	339089.713595	41.997543
3504.422298	339068.169045	42.002548
3504.484912	339066.428138	42.007552
3504.564364	339058.702445	42.012557
3504.409742	339041.518719	42.017562
3504.411526	339028.001363	42.022567
3504.651213	339030.738152	42.027572
3504.099043	339018.072039	42.032576
3504.173590	339002.659442	42.037581
3504.087643	339008.044206	42.042586
3504.260809	339009.518718	42.047591
3504.032693	338991.557464	42.052596
3504.154525	338981.355842	42.057600
3504.404356	338979.432602	42.062605
3504.543601	338984.425388	42.067610
3504.347158	338968.241032	42.072615
3504.132184	338962.496518	42.077620
3504.065970	338964.441621	42.082624
3504.347021	338962.462534	42.087629
3504.293560	338945.084599	42.092634
3504.131642	338934.545986	42.097639
3503.999436	338935.686934	42.102644
3504.090605	338944.225693	42.107648
3504.192844	338921.502856	42.112653
3503.901676	338918.443252	42.117658
3504.267825	338915.407019	42.122663
3504.310882	338918.098528	42.127668
3503.973015	338919.017427	42.132672
3504.092358	338895.579112	42.137677
3504.211454	338898.971367	42.142682
3504.155695	338889.485114	42.147687
3504.117845	338890.662058	42.152692
3504.312469	338891.751342	42.157696
3504.377158	338873.005547	42.162701
3504.229969	338883.618467	42.167706
3504.441159	338869.686137	42.172711
3504.400001	338853.197190	42.177716
3503.806199	338850.694541	42.182720
3504.027637	338841.393565	42.187725
3503.984192	338846.007946	42.192730
3504.031818	338854.375409	42.197735
3504.242290	338843.421531	42.202740
3504.095363	338832.218677	42.207744
3504.152004	338825.667535	42.212749
3503.981328	338829.029233	42.217754
3504.257410	338826.389073	42.222759
3504.311141	338814.798113	42.227764
3504.190494	338808.504098	42.232768
3504.273768	338798.766749	42.237773
3504.379735	338803.153867	42.242778
3504.190869	338793.128610	42.247783
3504.211751	338781.542837	42.252788
3504.137615	338786.671193	42.257792
3504.289112	338785.068964	42.262797
3504.240186	338778.458137	42.267802
3504.180157	338760.953911	42.272807
3504.341760	338750.338670	42.277812
3504.089773	338757.837093	42.282816
3504.275860	338737.213782	42.287821
3504.136925	338739.730420	42.292826
3503.970807	338735.556432	42.297831
3503.986651	338743.572549	42.302836
3503.653379	338753.909435	42.307840
3504.252003	338735.664683	42.312845
3503.840635	338724.478157	42.317850
3503.952988	338704.070140	42.322855
3504.504749	338712.103368	42.327860
3504.098293	338727.492112	42.332864
3504.075145	338701.352461	42.337869
3503.975034	338683.472710	42.342874
3504.399732	338692.518811	42.347879
3504.437380	338693.327440	42.352884
3503.950951	338681.847300	42.357888
3504.324628	338662.365288	42.362893
3503.965803	338671.102497	42.367898
3504.067683	338664.671468	42.372903
3504.223187	338665.817851	42.377908
3503.982101	338659.950157	42.382912
3504.079291	338641.097333	42.387917
3504.322451	338641.720740	42.392922
3504.111442	338640.048532	42.397927
3504.316427	338648.747530	42.402932
3504.170651	338632.020504	42.407936
3504.491125	338619.445470	42.412941
3504.106226	338612.251336	42.417946
3504.171203	338615.117585	42.422951
3504.424626	338605.862431	42.427956
3503.955858	338609.831295	42.432960
3504.152481	338600.330558	42.437965
3504.056698	338609.280755	42.442970
3504.123042	338594.327566	42.447975
3503.973133	338581.343218	42.452980
3504.042058	338588.307265	42.457984
3504.374750	338571.708237	42.462989
3503.899631	338587.820637	42.467994
3504.170316	338573.827927	42.472999
3504.324884	338558.122558	42.478004
3504.202766	338557.836378	42.483008
3504.105531	338547.567494	42.488013
3504.200863	338550.428947	42.493018
3504.056881	338531.614215	42.498023
3504.484626	338525.335308	42.503028
3504.119463	338529.185974	42.508032
3504.219647	338522.806111	42.513037
3504.121958	338510.704456	42.518042
3503.941081	338504.954510	42.523047
3504.139498	338503.446681	42.528052
3504.056512	338511.274802	42.533056
3504.514426	338505.271140	42.538061
3503.831104	338490.996467	42.543066
3504.371085	338482.230574	42.548071
3504.290129	338475.013834	42.553076
3503.784879	338485.123388	42.558080
3504.189809	338465.534552	42.563085
3504.147369	338456.657075	42.568090
3503.892703	338459.395667	42.573095
3504.166282	338447.948081	42.578100
3503.821792	338449.453523	42.583104
3504.110990	338445.207541	42.588109
3504.055203	338425.055120	42.593114
3503.935959	338425.455800	42.598119
3504.070725	338430.933003	42.603124
3503.544846	338431.983454	42.608128
3504.087891	338419.831408	42.613133
3504.045924	338429.765910	42.618138
3504.231186	338425.510900	42.623143
3504.161798	338414.626646	42.628148
3504.158389	338411.496073	42.633152
3504.335919	338404.467569	42.638157
3503.916855	338412.501564	42.643162
3504.469346	338381.001374	42.648167
3504.427039	338379.480684	42.653172
3504.013117	338384.764609	42.658176
3504.337391	338370.839752	42.663181
3504.127239	338365.348983	42.668186
3504.132958	338357.838511	42.673191
3504.383751	338346.267228	42.678196
3504.154072	338348.314559	42.683200
3504.178903	338325.705575	42.688205
3503.950043	338327.141829	42.693210
3503.822537	338326.831044	42.698215
3504.283751	338329.685581	42.703220
3503.716158	338342.910661	42.708224
3504.189231	338320.867220	42.713229
3503.888436	338317.274530	42.718234
3503.866379	338309.641162	42.723239
3504.098707	338310.928145	42.728244
3503.939250	338318.081061	42.733248
3504.302417	338303.182708	42.738253
3503.875560	338295.307855	42.743258
3504.045030	338279.701888	42.748263
3504.424770	338276.230723	42.753268
3503.859214	338290.779211	42.758272
3504.125068	338277.805447	42.763277
3504.062085	338274.226074	42.768282
3503.937302	338259.710319	42.773287
3504.115028	338260.573179	42.778292
3503.731146	338258.139148	42.783296
3503.855690	338262.727015	42.788301
3503.865788	338269.369466	42.793306
3503.916977	338262.259094	42.798311
3504.070864	338251.364973	42.803316
3503.871133	338247.094443	42.808321
3504.206096	338236.502626	42.813325
3504.364359	338235.357525	42.818330
3504.158310	338233.099030	42.823335
3504.075524	338226.137113	42.828340
3504.122609	338223.354936	42.833345
3504.245200	338221.451788	42.838349
3503.954161	338231.425694	42.843354
3503.888036	338230.086958	42.848359
3504.355237	338210.640939	42.853364
3504.090642	338213.304742	42.858369
3504.064063	338195.515058	42.863373
3504.218520	338196.356141	42.868378
3504.119449	338199.579271	42.873383
3504.384404	338184.187292	42.878388
3504.023799	338185.542551	42.883393
3504.351413	338162.147417	42.888397
3504.320571	338182.313591	42.893402
3504.204669	338150.562562	42.898407
3504.194293	338142.240011	42.903412
3503.843945	338141.913539	42.908417
3504.050795	338137.706011	42.913421
3504.176665	338142.802801	42.918426
3504.182919	338122.513198	42.923431
3503.823486	338120.202577	42.928436
3503.810925	338125.270339	42.933441
3504.156711	338112.767575	42.938445
3503.986984	338128.551794	42.943450
3503.822325	338120.279085	42.948455
3503.961911	338101.444859	42.953460
3503.629499	338092.842278	42.958465
3503.793129	338087.343311	42.963469
3504.082548	338092.210601	42.968474
3503.968853	338088.613778	42.973479
3504.049832	338096.212379	42.978484
3503.925707	338100.228617	42.983489
3504.242384	338078.286187	42.988493
3503.876915	338078.191211	42.993498
3503.942569	338076.882554	42.998503
3504.269984	338070.797657	43.003508
3504.132217	338075.325178	43.008513
3504.054618	338056.092516	43.013517
3503.923665	338046.516201	43.018522
3503.760526	338042.239872	43.023527
3503.771939	338043.739976	43.028532
3503.587206	338052.653398	43.033537
3504.009199	338043.116954	43.038541
3503.678684	338054.319027	43.043546
3504.093011	338054.508082	43.048551
3504.073922	338058.125875	43.053556
3503.803249	338034.723447	43.058561
3504.034544	338021.195058	43.063565
3503.948543	338032.333026	43.068570
3504.134548	338028.841560	43.073575
3504.208744	338036.008484	43.078580
3503.848481	338023.617315	43.083585
3504.019962	338005.592619	43.088589
3503.665579	338004.452184	43.093594
3503.701092	338005.973935	43.098599
3503.586721	338004.031872	43.103604
3503.487137	338011.811763	43.108609
3503.607106	338011.360031	43.113613
3503.973765	338018.888025	43.118618
3503.683220	338009.846058	43.123623
3504.048674	338016.050516	43.128628
3504.012546	338018.398192	43.133633
3504.167759	338015.573457	43.138637
3503.953186	337999.773569	43.143642
3503.905190	337988.605843	43.148647
3503.949867	337992.620860	43.153652
3503.963389	337994.706126	43.158657
3504.115348	337988.623501	43.163661
3504.291074	337989.995806	43.168666
3504.175558	337960.179300	43.173671
3504.126569	337960.594334	43.178676
3503.606612	337966.531462	43.183681
3503.932115	337962.712466	43.188685
3503.924694	337972.590664	43.193690
3503.886706	337969.567361	43.198695
3504.397869	337952.176274	43.203700
3503.885485	337942.227483	43.208705
3504.145084	337936.840614	43.213709
3503.908270	337941.511083	43.218714
3503.957661	337937.124783	43.223719
3504.391221	337934.001480	43.228724
3504.160616	337917.924088	43.233729
3504.303609	337899.598391	43.238733
3504.423338	337907.700015	43.243738
3503.986687	337894.506294	43.248743
3504.328744	337885.135202	43.253748
3504.067565	337881.994439	43.258753
3504.301972	337880.760926	43.263757
3503.964309	337871.293631	43.268762
3503.776012	337858.518857	43.273767
3504.089751	337855.516317	43.278772
3503.973447	337851.461680	43.283777
3504.026517	337851.580561	43.288781
3503.768631	337861.091068	43.293786
3503.838497	337856.548788	43.298791
3504.255844	337857.831988	43.303796
3504.141028	337847.743966	43.308801
3504.117996	337844.107341	43.313805
3504.184381	337842.951302	43.318810
3504.164831	337840.968787	43.323815
3504.283602	337813.355335	43.328820
3503.794356	337818.116630	43.333825
3504.040654	337809.575267	43.338829
3503.892932	337815.326284	43.343834
3504.187219	337823.527606	43.348839
3503.832119	337807.724430	43.353844
3503.974748	337801.286874	43.358849
3503.845431	337776.003695	43.363853
3503.794329	337784.030513	43.368858
3503.931809	337781.615872	43.373863
3504.121984	337781.254866	43.378868
3504.003486	337791.863428	43.383873
3503.853486	337775.238676	43.388877
3503.782163	337760.357971	43.393882
3503.779490	337754.223399	43.398887
3503.750535	337760.821163	43.403892
3503.544442	337755.482439	43.408897
3503.798454	337752.260228	43.413901
3503.722773	337757.210715	43.418906
3503.759429	337762.041618	43.423911
3503.960822	337762.951656	43.428916
3503.745072	337761.534738	43.433921
3503.828735	337763.176165	43.438925
3503.945570	337778.813344	43.443930
3503.886960	337773.018549	43.448935
3503.704052	337757.748181	43.453940
3503.842981	337755.027834	43.458945
3504.092630	337742.667478	43.463949
3503.920628	337748.040494	43.468954
3503.911549	337749.722038	43.473959
3504.087300	337749.796070	43.478964
3503.745698	337752.599346	43.483969
3503.854406	337754.720485	43.488973
3503.613764	337734.953462	43.493978
3503.704612	337721.930884	43.498983
3504.028954	337724.908910	43.503988
3503.932328	337718.127321	43.508993
3503.829103	337725.755084	43.513997
3503.847773	337733.898160	43.519002
3503.914582	337733.989414	43.524007
3504.152164	337727.944142	43.529012
3503.962761	337731.334313	43.534017
3504.005559	337715.519128	43.539021
3504.072948	337705.911410	43.544026
3504.262589	337708.248864	43.549031
3504.103159	337701.502658	43.554036
3503.910677	337705.147880	43.559041
3503.903025	337672.539447	43.564045
3504.138644	337678.917200	43.569050
3503.984851	337674.970304	43.574055
3503.954877	337664.843386	43.579060
3503.835741	337676.419411	43.584065
3504.118852	337676.985599	43.589069
3503.936981	337668.333708	43.594074
3503.960408	337654.150780	43.599079
3504.224921	337650.137756	43.604084
3503.888598	337649.350850	43.609089
3504.183750	337649.940591	43.614093
3504.288633	337652.189620	43.619098
3503.710847	337630.464805	43.624103
3504.068514	337629.568193	43.629108
3504.068483	337616.279940	43.634113
3504.300512	337612.348418	43.639117
3504.206043	337626.237086	43.644122
3503.766170	337590.209409	43.649127
3503.933073	337577.862103	43.654132
3503.653288	337584.015863	43.659137
3503.867147	337576.116008	43.664141
3503.928540	337592.602057	43.669146
3503.832451	337595.086509	43.674151
3504.010652	337587.039554	43.679156
3503.935920	337594.331895	43.684161
3503.715628	337573.339698	43.689165
3503.887466	337564.224576	43.694170
3503.659926	337562.402214	43.699175
3503.647135	337559.629474	43.704180
3503.548396	337562.979865	43.709185
3503.762481	337558.516591	43.714189
3503.825006	337557.539352	43.719194
3503.794661	337568.134015	43.724199
3504.170766	337570.798388	43.729204
3503.618287	337580.024571	43.734209
3503.809634	337573.477466	43.739213
3503.782833	337591.301191	43.744218
3503.792143	337578.978798	43.749223
3504.021138	337553.817086	43.754228
3503.621103	337559.480729	43.759233
3503.629674	337550.798717	43.764237
3503.552624	337556.564042	43.769242
3503.639072	337557.135863	43.774247
3503.975969	337553.060478	43.779252
3503.966650	337558.255054	43.784257
3504.304808	337552.270237	43.789261
3504.383078	337562.084038	43.794266
3504.224955	337541.387480	43.799271
3504.292403	337535.470912	43.804276
3503.956404	337533.563869	43.809281
3504.160423	337519.785124	43.814285
3504.239258	337507.324444	43.819290
3503.890760	337496.636898	43.824295
3503.902069	337496.405991	43.829300
3503.751650	337510.023507	43.834305
3503.990375	337499.726806	43.839309
3504.063668	337507.632167	43.844314
3503.899174	337482.099871	43.849319
3503.998266	337472.334368	43.854324
3503.574116	337467.921068	43.859329
3503.476964	337470.125671	43.864333
3504.013997	337463.931213	43.869338
3504.055189	337466.928554	43.874343
3503.866223	337469.656800	43.879348
3503.901555	337478.382773	43.884353
3504.386805	337468.123466	43.889357
3504.190940	337455.477093	43.894362
3504.110151	337460.606605	43.899367
3504.426876	337458.749116	43.904372
3503.971643	337458.591960	43.909377
3503.845922	337422.820007	43.914381
3503.825180	337420.124887	43.919386
3503.630666	337421.810297	43.924391
3503.978424	337422.697203	43.929396
3503.791067	337426.137978	43.934401
3504.217179	337414.767926	43.939405
3504.082814	337422.960689	43.944410
3503.705168	337411.081281	43.949415
3503.882996	337391.629851	43.954420
3503.488574	337388.790149	43.959425
3503.753414	337385.540752	43.964429
3503.652840	337387.262226	43.969434
3503.535262	337397.107011	43.974439
3503.660625	337391.003079	43.979444
3503.903703	337393.637575	43.984449
3504.012711	337393.416680	43.989453
3503.736390	337406.290425	43.994458
3503.832166	337412.257550	43.999463
3503.923172	337402.773336	44.004468
3503.956569	337402.462568	44.009473
3503.997774	337398.510286	44.014477
3503.933314	337382.050108	44.019482
3503.676903	337379.875914	44.024487
3503.939656	337377.899673	44.029492
3503.929446	337379.403209	44.034497
3503.873910	337376.509936	44.039501
3503.795827	337385.101111	44.044506
3503.759468	337387.168824	44.049511
3504.197576	337377.782476	44.054516
3503.758557	337370.698586	44.059521
3504.088550	337356.925350	44.064525
3504.070256	337356.189992	44.069530
3503.875067	337349.449402	44.074535
3503.825532	337349.431765	44.079540
3503.765967	337357.052669	44.084545
3503.756094	337363.087412	44.089549
3503.753230	337367.950048	44.094554
3503.772651	337351.018385	44.099559
3504.499632	337321.602995	44.104564
3504.080634	337325.131306	44.109569
3503.976451	337326.649700	44.114573
3504.379101	337329.411712	44.119578
3504.186811	337309.458723	44.124583
3504.135794	337299.716923	44.129588
3503.919347	337300.616650	44.134593
3504.173116	337299.023675	44.139597
3504.068514	337296.138154	44.144602
3503.829963	337282.022016	44.149607
3503.954541	337273.958043	44.154612
3503.922311	337270.399210	44.159617
3503.654111	337267.819572	44.164621
3503.590061	337269.637101	44.169626
3503.590558	337266.887704	44.174631
3503.689855	337266.261039	44.179636
3503.919824	337271.748745	44.184641
3503.923426	337264.925810	44.189645
3503.770756	337276.914510	44.194650
3503.920361	337279.436504	44.199655
3504.250167	337253.978721	44.204660
3503.814869	337257.636896	44.209665
3503.650215	337241.167064	44.214669
3503.645054	337246.361007	44.219674
3503.903038	337250.978764	44.224679
3503.958712	337257.232265	44.229684
3503.593027	337262.508654	44.234689
3503.721265	337266.535963	44.239693
3503.854445	337258.037867	44.244698
3503.904570	337263.248526	44.249703
3503.946593	337229.079171	44.254708
3504.048342	337232.296059	44.259713
3504.084654	337221.267615	44.264717
3504.029188	337235.277483	44.269722
3503.868377	337221.174499	44.274727
3504.146090	337220.468717	44.279732
3503.729947	337205.184177	44.284737
3503.939615	337189.775250	44.289741
3503.996129	337192.235593	44.294746
3503.784961	337197.105713	44.299751
3503.890659	337186.779079	44.304756
3503.913256	337199.681981	44.309761
3503.949983	337201.254472	44.314765
3504.297112	337196.795599	44.319770
3503.842109	337174.873029	44.324775
3504.168629	337163.213198	44.329780
3503.630437	337162.763676	44.334785
3503.751713	337155.922127	44.339789
3503.964794	337159.910574	44.344794
3503.680806	337160.464587	44.349799
3503.950000	337162.585832	44.354804
3503.753273	337159.434846	44.359809
3503.917227	337150.295457	44.364813
3504.107486	337142.246542	44.369818
3503.942848	337138.352241	44.374823
3504.012655	337140.199526	44.379828
3503.348560	337154.127426	44.384833
3503.593995	337150.041019	44.389837
3503.973191	337145.500704	44.394842
3503.491515	337155.173972	44.399847
3503.696284	337153.486913	44.404852
3503.837594	337160.388757	44.409857
3503.895935	337153.149851	44.414861
3503.666383	337131.700759	44.419866
3503.610977	337126.720012	44.424871
3503.841347	337119.632105	44.429876
3503.541582	337126.450937	44.434881
3503.367356	337121.336234	44.439885
3503.905558	337119.036419	44.444890
3504.152476	337122.153995	44.449895
3504.152733	337125.437845	44.454900
3503.995608	337132.208672	44.459905
3503.937648	337133.617936	44.464909
3504.026600	337127.876128	44.469914
3503.839304	337107.285873	44.474919
3504.210772	337101.855795	44.479924
3503.658014	337110.878435	44.484929
3503.680562	337108.736504	44.489933
3503.772533	337109.129260	44.494938
3503.911554	337110.049167	44.499943
3504.144913	337108.510327	44.504948
3504.097963	337102.688174	44.509953
3504.274624	337076.185354	44.514957
3503.969024	337084.914359	44.519962
3503.821018	337088.578042	44.524967
3504.210433	337080.523093	44.529972
3503.872461	337077.827194	44.534977
3503.872716	337061.585815	44.539981
3504.262989	337047.192027	44.544986
3503.816196	337048.739129	44.549991
3503.944586	337055.057524	44.554996
3503.803887	337060.247450	44.560001
3503.958247	337055.564475	44.565005
3503.782331	337066.869559	44.570010
3503.892977	337050.305248	44.575015
3503.778524	337030.849002	44.580020
3503.793004	337026.442703	44.585025
3503.850169	337026.026349	44.590029
3503.842056	337027.504106	44.595034
3503.791454	337027.843030	44.600039
3503.763043	337025.429130	44.605044
3503.789752	337027.690538	44.610049
3503.966356	337024.582355	44.615053
3503.966298	337032.753935	44.620058
3503.831381	337019.105035	44.625063
3504.165104	337004.720177	44.630068
3503.755653	337010.792661	44.635073
3503.996632	337001.488335	44.640077
3504.031466	337000.260898	44.645082
3503.812222	337001.619291	44.650087
3503.944561	336996.914336	44.655092
3503.742015	337013.289513	44.660097
3504.005429	336979.441425	44.665101
3503.582893	336977.624416	44.670106
3503.646828	336974.508585	44.675111
3504.116861	336961.476830	44.680116
3503.730484	336984.245240	44.685121
3503.786457	336975.555660	44.690125
3503.845809	336981.274015	44.695130
3503.881193	336974.802418	44.700135
3504.087445	336982.839565	44.705140
3503.867240	336971.164299	44.710145
3503.956865	336956.843474	44.715149
3503.567971	336958.228686	44.720154
3503.368934	336959.838452	44.725159
3503.592860	336953.693442	44.730164
3503.495679	336957.832774	44.735169
3503.547880	336958.639125	44.740173
3503.579264	336958.226846	44.745178
3503.796885	336964.785710	44.750183
3504.258491	336968.302118	44.755188
3504.067425	336969.172381	44.760193
3503.822737	336964.985243	44.765197
3504.016372	336961.899823	44.770202
3503.516353	336954.010917	44.775207
3503.535701	336947.898247	44.780212
3503.596527	336954.532811	44.785217
3503.599762	336967.795213	44.790221
3503.899222	336963.114750	44.795226
3503.570249	336948.045481	44.800231
3503.696968	336940.515720	44.805236
3503.675292	336948.054311	44.810241
3503.807400	336938.028943	44.815245
3503.789627	336936.504341	44.820250
3503.494108	336952.639663	44.825255
3504.024780	336949.780987	44.830260
3503.604806	336945.341534	44.835265
3503.909097	336937.121828	44.840269
3503.838633	336945.508202	44.845274
3503.596586	336956.849216	44.850279
3503.919013	336950.128588	44.855284
3503.642365	336959.718560	44.860289
3503.674590	336955.513105	44.865293
3503.836449	336938.838844	44.870298
3503.393454	336939.672561	44.875303
3503.717499	336922.310784	44.880308
3503.816899	336925.935365	44.885313
3503.815880	336926.113712	44.890317
3503.644148	336926.039021	44.895322
3503.931479	336927.139140	44.900327
3504.023900	336922.440490	44.905332
3503.691756	336936.112307	44.910337
3503.973518	336924.230400	44.915341
3503.802432	336934.516476	44.920346
3503.590697	336942.136025	44.925351
3503.873359	336927.631938	44.930356
3503.803307	336921.533397	44.935361
3503.645365	336918.834489	44.940365
3503.634015	336904.427788	44.945370
3503.752056	336903.747243	44.950375
3503.731625	336896.800785	44.955380
3503.557851	336903.599724	44.960385
3503.655017	336908.090187	44.965389
3503.584760	336907.973998	44.970394
3503.583660	336915.203860	44.975399
3503.638402	336909.009221	44.980404
3503.464675	336913.847986	44.985409
3503.816959	336916.694348	44.990413
3503.836415	336916.716718	44.995418
3503.809272	336918.681163	45.000423
3504.205557	336917.854806	45.005428
3503.730607	336916.707954	45.010433
3504.103578	336917.819992	45.015437
3503.710069	336900.367986	45.020442
3503.630156	336896.613017	45.025447
3504.183392	336892.325197	45.030452
3504.094671	336887.426069	45.035457
3503.967892	336882.863893	45.040461
3504.103262	336894.985327	45.045466
3503.761321	336888.853393	45.050471
3503.855483	336867.658523	45.055476
3503.489434	336867.818204	45.060481
3503.638371	336863.161529	45.065485
3503.996062	336863.486825	45.070490
3504.042151	336860.322897	45.075495
3503.826868	336861.349729	45.080500
3503.878472	336864.319995	45.085505
3503.936531	336864.438089	45.090509
3504.078417	336864.797500	45.095514
3503.602783	336853.977206	45.100519
3503.700233	336838.509567	45.105524
3503.514318	336830.316426	45.110529
3503.588103	336826.766268	45.115533
3503.714611	336835.936133	45.120538
3503.752400	336837.788488	45.125543
3504.166108	336835.762912	45.130548
3504.040462	336845.863621	45.135553
3504.074573	336845.730934	45.140557
3503.878850	336841.688789	45.145562
3503.588402	336845.731396	45.150567
3504.016609	336836.855671	45.155572
3503.731887	336830.332836	45.160577
3503.955519	336820.853031	45.165581
3503.948516	336813.089827	45.170586
3503.921625	336809.631952	45.175591
3504.003377	336808.498922	45.180596
3503.912967	336812.458995	45.185601
3504.021823	336809.947017	45.190605
3503.788619	336797.179137	45.195610
3503.551043	336791.667115	45.200615
3503.885298	336777.103926	45.205620
3504.030332	336791.591327	45.210625
3504.047912	336786.268080	45.215629
3504.021718	336780.493530	45.220634
3503.693350	336791.593650	45.225639
3503.752779	336795.937346	45.230644
3503.738878	336794.844893	45.235649
3504.087113	336771.700574	45.240653
3504.057400	336757.398571	45.245658
3503.553323	336756.918196	45.250663
3504.017785	336743.505427	45.255668
3503.707739	336750.784145	45.260673
3504.061611	336749.964491	45.265677
3504.228453	336754.087556	45.270682
3503.667171	336747.048383	45.275687
3503.606895	336729.289087	45.280692
3503.687980	336718.457136	45.285697
3503.781165	336721.420835	45.290701
3503.698727	336719.600969	45.295706
3503.622563	336732.214093	45.300711
3503.815737	336718.487810	45.305716
3503.973300	336732.260454	45.310721
3503.849721	336734.189234	45.315725
3503.907462	336729.750620	45.320730
3503.997283	336733.402183	45.325735
3503.977969	336726.022766	45.330740
3503.430328	336726.032956	45.335745
3503.880590	336714.608053	45.340749
3503.810874	336713.040743	45.345754
3503.581614	336707.527399	45.350759
3504.019893	336697.249942	45.355764
3503.448782	336697.543866	45.360769
3503.523687	336705.525439	45.365773
3503.933063	336706.911750	45.370778
3503.895541	336708.852384	45.375783
3503.770527	336704.137177	45.380788
3503.921833	336705.971591	45.385793
3503.796672	336700.849099	45.390797
3503.690096	336709.775803	45.395802
3503.882134	336706.588796	45.400807
3504.149813	336699.036725	45.405812
3503.727891	336684.949447	45.410817
3503.828325	336685.748176	45.415821
3503.781009	336679.849673	45.420826
3503.817047	336687.506454	45.425831
3504.206583	336686.197484	45.430836
3503.816303	336685.902773	45.435841
3503.772477	336680.385570	45.440845
3503.851554	336673.856124	45.445850
3503.446971	336661.217137	45.450855
3503.804003	336648.050443	45.455860
3503.764620	336652.180657	45.460865
3503.777083	336655.869909	45.465869
3503.682183	336654.662974	45.470874
3503.773969	336655.335787	45.475879
3503.852270	336650.613893	45.480884
3504.001516	336664.387865	45.485889
3503.839933	336648.935673	45.490893
3504.066365	336656.002311	45.495898
3503.862074	336657.383803	45.500903
3503.889782	336632.304477	45.505908
3503.845179	336628.594825	45.510913
3503.726960	336632.482934	45.515917
3503.955129	336626.209940	45.520922
3503.641593	336630.587147	45.525927
3503.907402	336626.497487	45.530932
3503.667153	336630.073949	45.535937
3503.797235	336639.497844	45.540941
3503.852641	336633.557642	45.545946
3503.544380	336637.501250	45.550951
3503.872753	336639.409503	45.555956
3504.022267	336628.210325	45.560961
3503.843138	336600.287065	45.565965
3504.118178	336606.149554	45.570970
3504.166818	336597.231973	45.575975
3504.010572	336594.481869	45.580980
3503.913978	336605.290813	45.585985
3503.853815	336590.509908	45.590989
3504.006769	336574.727952	45.595994
3503.511634	336575.188064	45.600999
3503.593626	336575.582401	45.606004
3503.769237	336579.016756	45.611009
3503.495409	336579.925563	45.616013
3503.410477	336575.585863	45.621018
3503.799364	336581.557642	45.626023
3503.958172	336578.324968	45.631028
3503.856871	336581.777640	45.636033
3503.744285	336579.020634	45.641037
3504.006285	336580.073849	45.646042
3503.725980	336579.456272	45.651047
3503.816032	336578.347382	45.656052
3504.058310	336558.885521	45.661057
3503.894198	336546.004843	45.666061
3503.797244	336553.580836	45.671066
3503.914778	336546.739816	45.676071
3504.093734	336540.067284	45.681076
3503.628078	336554.447619	45.686081
3503.698611	336552.043517	45.691085
3504.137880	336552.865055	45.696090
3503.974179	336545.661184	45.701095
3503.772574	336533.524679	45.706100
3503.862176	336529.946548	45.711105
3503.838221	336522.669669	45.716109
3503.931486	336518.581821	45.721114
3503.635787	336531.840651	45.726119
3504.132023	336525.092505	45.731124
3503.874448	336532.872088	45.736129
3503.738691	336523.016287	45.741133
3503.750481	336500.637851	45.746138
3503.738097	336496.617616	45.751143
3503.715889	336489.213174	45.756148
3503.581722	336495.216731	45.761153
3503.800343	336491.440004	45.766157
3503.917704	336493.050679	45.771162
3503.657043	336497.317709	45.776167
3503.999811	336488.124506	45.781172
3503.607573	336497.096395	45.786177
3503.421140	336506.697628	45.791181
3503.825540	336496.094557	45.796186
3503.805546	336491.006338	45.801191
3503.704925	336499.728474	45.806196
3503.577420	336504.458134	45.811201
3504.058647	336503.440148	45.816205
3504.031601	336493.287132	45.821210
3503.475357	336479.246501	45.826215
3503.938734	336473.776387	45.831220
3503.828554	336474.302930	45.836225
3503.538926	336475.214237	45.841229
3503.550916	336465.131416	45.846234
3503.510196	336480.106472	45.851239
3503.778857	336474.845336	45.856244
3503.709202	336488.933974	45.861249
3503.627021	336483.575559	45.866253
3503.684451	336478.347815	45.871258
3503.527986	336491.050049	45.876263
3503.821701	336479.955335	45.881268
3503.808626	336489.580080	45.886273
3503.847168	336488.402961	45.891277
3503.892414	336484.628184	45.896282
3503.757664	336480.805490	45.901287
3503.879815	336460.038834	45.906292
3503.668196	336455.515498	45.911297
3503.769501	336443.025610	45.916301
3503.898643	336441.274118	45.921306
3503.657746	336457.171812	45.926311
3503.829952	336452.536887	45.931316
3503.642339	336456.996028	45.936321
3503.435105	336455.908674	45.941325
3503.611870	336460.742980	45.946330
3503.551055	336458.919689	45.951335
3503.827876	336459.563254	45.956340
3503.441444	336466.039458	45.961345
3503.602056	336466.370453	45.966349
3503.701092	336462.358060	45.971354
3503.767627	336466.013318	45.976359
3503.822016	336462.873516	45.981364
3503.661418	336466.717421	45.986369
3503.969271	336460.660926	45.991373
3503.762454	336471.538229	45.996378
3503.624881	336444.906635	46.001383
3503.596751	336435.135634	46.006388
3503.449614	336443.152338	46.011393
3503.706969	336434.863620	46.016397
3503.890414	336435.878342	46.021402
3503.510961	336450.677839	46.026407
3503.748857	336434.704224	46.031412
3503.824174	336443.322185	46.036417
3503.619572	336446.434798	46.041421
3503.818944	336438.435271	46.046426
3504.024841	336449.527362	46.051431
3503.825880	336449.762457	46.056436
3503.800903	336458.523555	46.061441
3504.293170	336443.298894	46.066445
3503.969858	336427.210338	46.071450
3503.879122	336417.805628	46.076455
3503.857725	336416.103389	46.081460
3503.738930	336418.973326	46.086465
3503.994618	336411.321291	46.091469
3503.853690	336406.150355	46.096474
3503.773213	336414.589292	46.101479
3503.791750	336410.335052	46.106484
3503.591752	336408.991985	46.111489
3503.760102	336403.899443	46.116493
3504.027129	336396.703837	46.121498
3503.547426	336392.681099	46.126503
3503.793495	336383.223142	46.131508
3503.606193	336396.032095	46.136513
3503.595376	336386.487463	46.141517
3503.638660	336385.055024	46.146522
3503.573865	336393.669683	46.151527
3503.712545	336395.735213	46.156532
3503.605529	336395.879404	46.161537
3503.701376	336393.547665	46.166541
3503.990944	336400.706177	46.171546
3503.514269	336399.024994	46.176551
3503.729480	336395.376085	46.181556
3503.658365	336401.598795	46.186561
3503.979026	336407.632288	46.191565
3504.242411	336407.845210	46.196570
3503.289448	336386.993915	46.201575
3503.966087	336363.924827	46.206580
3503.649442	336375.532300	46.211585
3503.873678	336375.216816	46.216589
3503.976704	336368.938123	46.221594
3503.755294	336363.499881	46.226599
3503.945951	336363.036963	46.231604
3503.685311	336369.162352	46.236609
3503.672915	336362.010913	46.241613
3504.073706	336361.285666	46.246618
3503.754050	336373.046357	46.251623
3503.937829	336348.985985	46.256628
3503.689215	336342.559222	46.261633
3503.743403	336339.724929	46.266637
3503.823770	336331.871486	46.271642
3503.807188	336341.140410	46.276647
3503.907896	336340.895367	46.281652
3503.975792	336337.447941	46.286657
3503.976309	336344.117557	46.291661
3503.832945	336347.678718	46.296666
3503.853503	336332.172203	46.301671
3503.996529	336306.234447	46.306676
3503.760060	336316.683695	46.311681
3503.815877	336313.900057	46.316685
3504.045717	336311.394392	46.321690
3503.778752	336313.244023	46.326695
3504.028050	336308.342333	46.331700
3503.913314	336311.364375	46.336705
3504.025807	336304.600499	46.341709
3503.556560	336289.145945	46.346714
3503.554054	336290.317349	46.351719
3503.918086	336287.332246	46.356724
3503.665438	336294.576482	46.361729
3503.534709	336286.552749	46.366733
3503.759171	336289.673914	46.371738
3503.811614	336296.411696	46.376743
3503.817950	336293.635880	46.381748
3503.608451	336297.869378	46.386753
3503.547177	336302.410384	46.391757
3503.886646	336301.363890	46.396762
3503.602692	336306.907461	46.401767
3503.753910	336301.944903	46.406772
3503.761526	336306.678675	46.411777
3503.702782	336298.567194	46.416781
3504.182236	336301.495307	46.421786
3503.985869	336282.051793	46.426791
3503.977585	336269.299170	46.431796
3503.833036	336270.874882	46.436801
3504.055335	336276.643910	46.441805
3504.099850	336275.236731	46.446810
3503.774655	336274.600790	46.451815
3503.666180	336244.196890	46.456820
3503.782328	336233.155663	46.461825
3503.525171	336235.894739	46.466829
3503.379614	336241.518265	46.471834
3503.315762	336238.626256	46.476839
3503.691144	336249.309734	46.481844
3503.843850	336240.833879	46.486849
3503.926287	336236.773183	46.491853
3503.996103	336234.827408	46.496858
3503.563104	336243.194808	46.501863
3503.625167	336234.096858	46.506868
3503.843140	336235.080667	46.511873
3503.751874	336232.778502	46.516877
3503.756248	336229.824794	46.521882
3503.763065	336239.548257	46.526887
3503.864395	336233.320734	46.531892
3503.683577	336246.383261	46.536897
3503.910152	336246.932942	46.541901
3503.699249	336222.425777	46.546906
3503.758729	336216.612180	46.551911
3503.854044	336211.938479	46.556916
3503.854378	336206.286972	46.561921
3504.016364	336207.686944	46.566925
3504.142555	336194.658480	46.571930
3504.018169	336207.890292	46.576935
3503.920553	336197.570188	46.581940
3503.505142	336189.998757	46.586945
3503.756259	336184.231234	46.591949
3503.888510	336172.729226	46.596954
3503.743389	336180.211046	46.601959
3503.990020	336183.761479	46.606964
3503.908330	336182.068765	46.611969
3503.850962	336181.950538	46.616973
3504.070079	336178.682855	46.621978
3503.971461	336186.259151	46.626983
3504.098741	336164.651513	46.631988
3503.820656	336155.632780	46.636993
3503.741352	336150.324798	46.641997
3503.968730	336145.248362	46.647002
3503.747264	336155.644349	46.652007
3504.203262	336144.345728	46.657012
3503.920887	336150.016346	46.662017
3504.014082	336134.065535	46.667021
3503.730218	336116.163223	46.672026
3503.731442	336114.202830	46.677031
3503.790922	336110.909465	46.682036
3503.626434	336121.907418	46.687041
3503.379212	336114.003907	46.692045
3503.706320	336108.377106	46.697050
3503.593082	336118.577792	46.702055
3503.639701	336115.871970	46.707060
3503.825683	336108.001807	46.712065
3503.785098	336122.773264	46.717069
3503.873939	336126.017703	46.722074
3504.086981	336130.693557	46.727079
3504.283873	336113.224386	46.732084
3504.027931	336093.332009	46.737089
3503.726190	336092.437788	46.742093
3504.145954	336082.494105	46.747098
3503.949412	336089.143984	46.752103
3504.246596	336079.092393	46.757108
3503.704888	336075.155808	46.762113
3503.935027	336057.706825	46.767117
3503.732358	336052.851105	46.772122
3503.701622	336062.147762	46.777127
3503.920903	336051.701170	46.782132
3503.688005	336058.000400	46.787137
3503.440356	336063.971020	46.792141
3503.985149	336046.014067	46.797146
3503.856904	336056.904473	46.802151
3503.796142	336061.929098	46.807156
3503.929580	336061.857079	46.812161
3504.047824	336053.310277	46.817165
3504.291126	336034.815469	46.822170
3504.089752	336022.958863	46.827175
3504.146866	336020.098637	46.832180
3504.015378	336033.382519	46.837185
3503.770768	336020.259896	46.842189
3503.879584	335998.909694	46.847194
3503.936179	335989.277978	46.852199
3503.722807	335993.079338	46.857204
3503.559371	335998.705710	46.862209
3503.828161	335993.877286	46.867213
3503.671873	335994.971177	46.872218
3503.338586	335998.409637	46.877223
3503.891147	335990.099655	46.882228
3503.639681	335989.884826	46.887233
3503.337730	335995.609466	46.892237
3503.856332	335996.545755	46.897242
3503.931943	336000.937858	46.902247
3503.888520	335999.850059	46.907252
3503.675031	336001.309390	46.912257
3503.573484	335996.946822	46.917261
3503.874484	336000.641413	46.922266
3503.573306	335997.634168	46.927271
3503.703843	335988.729017	46.932276
3503.918156	335975.101069	46.937281
3503.708006	335972.130347	46.942285
3503.467298	335967.586120	46.947290
3503.360445	335973.152635	46.952295
3503.693320	335968.237708	46.957300
3503.698471	335965.996663	46.962305
3503.790113	335973.186509	46.967309
3503.918911	335965.656309	46.972314
3503.858687	335969.866231	46.977319
3503.972638	335964.044001	46.982324
3503.923799	335979.351392	46.987329
3504.076483	335976.577885	46.992333
3503.946187	335963.488094	46.997338
3503.850512	335948.967233	47.002343
3503.779899	335939.941131	47.007348
3503.834598	335940.110672	47.012353
3503.895338	335934.907820	47.017357
3503.925314	335941.038220	47.022362
3503.262547	335948.550982	47.027367
3503.412480	335939.235445	47.032372
3503.368300	335946.854077	47.037377
3503.435095	335951.374862	47.042381
3503.729897	335941.781854	47.047386
3503.790088	335953.788056	47.052391
3503.819949	335944.975186	47.057396
3503.576010	335945.955647	47.062401
3503.994045	335955.639604	47.067405
3503.907790	335945.114009	47.072410
3503.503642	335954.495166	47.077415
3503.959904	335945.945831	47.082420
3503.778874	335941.061226	47.087425
3503.749317	335930.933980	47.092429
3503.936081	335918.099544	47.097434
3503.346391	335916.308928	47.102439
3503.631940	335912.547046	47.107444
3503.367004	335922.033486	47.112449
3503.220760	335913.579392	47.117453
3503.510754	335926.389355	47.122458
3503.422831	335924.061193	47.127463
3503.387865	335939.137287	47.132468
3503.858811	335963.145199	47.137473
3503.595666	335948.498069	47.142477
3503.526183	335939.649987	47.147482
3503.575800	335936.179973	47.152487
3503.447241	335941.877208	47.157492
3503.576405	335961.509621	47.162497
3503.660895	335968.827883	47.167501
3504.010034	335959.429944	47.172506
3503.361224	335953.982860	47.177511
3503.423977	335936.280278	47.182516
3503.154908	335952.029803	47.187521
3503.255663	335966.829866	47.192525
3503.878082	335972.993896	47.197530
3503.645625	335980.515001	47.202535
3503.777169	335975.122760	47.207540
3503.801073	335981.635973	47.212545
3503.630003	335962.290195	47.217549
3503.965026	335944.671860	47.222554
3503.635472	335946.862337	47.227559
3503.865560	335937.050445	47.232564
3503.838008	335940.262379	47.237569
3503.547159	335939.875575	47.242573
3503.887607	335936.715985	47.247578
3503.621402	335946.864506	47.252583
3503.775891	335947.654699	47.257588
3503.620081	335956.843856	47.262593
3503.527395	335957.953150	47.267597
3503.769226	335947.986661	47.272602
3503.849519	335958.513176	47.277607
3503.917226	335955.982214	47.282612
3503.757209	335950.126920	47.287617
3503.709647	335936.413076	47.292621
3503.680363	335925.242046	47.297626
3503.590273	335918.637441	47.302631
3503.668337	335921.832679	47.307636
3503.728392	335919.557496	47.312641
3503.586704	335918.688886	47.317645
3503.868178	335917.320612	47.322650
3503.730848	335926.226824	47.327655
3503.998022	335921.958707	47.332660
3503.736534	335925.589477	47.337665
3503.846544	335926.997671	47.342669
3503.800610	335925.935725	47.347674
3503.604115	335928.105169	47.352679
3503.735617	335924.036697	47.357684
3503.688510	335931.681251	47.362689
3503.676361	335929.824795	47.367693
3504.176595	335909.456429	47.372698
3503.645891	335906.485463	47.377703
3503.741068	335890.050597	47.382708
3503.848983	335886.444079	47.387713
3503.860437	335894.181208	47.392717
3503.922907	335891.396500	47.397722
3503.530575	335892.324050	47.402727
3503.715417	335895.629695	47.407732
3503.641140	335897.194307	47.412737
3503.599565	335900.866686	47.417741
3503.872714	335903.292832	47.422746
3503.734671	335904.460210	47.427751
3503.886666	335902.730548	47.432756
3503.741347	335885.315416	47.437761
3503.894014	335875.006612	47.442765
3503.746808	335868.640144	47.447770
3503.906163	335880.325199	47.452775
3503.966676	335876.726174	47.457780
3503.974091	335876.724991	47.462785
3503.863818	335883.692193	47.467789
3504.041355	335872.870317	47.472794
3503.860279	335862.385155	47.477799
3503.584014	335847.460050	47.482804
3503.391431	335839.293299	47.487809
3503.679242	335840.291532	47.492813
3503.990566	335842.202503	47.497818
3503.666103	335839.198932	47.502823
3504.024695	335838.785835	47.507828
3503.872784	335839.548094	47.512833
3503.904697	335849.674960	47.517837
3504.071136	335844.328107	47.522842
3504.136315	335839.328202	47.527847
3503.831120	335817.839733	47.532852
3503.512013	335814.911686	47.537857
3503.576645	335811.999348	47.542861
3503.540640	335808.491949	47.547866
3503.525575	335814.833137	47.552871
3503.749194	335804.742221	47.557876
3503.871245	335808.694224	47.562881
3503.733500	335820.120770	47.567885
3504.028738	335822.467055	47.572890
3504.058762	335814.035997	47.577895
3504.087316	335811.613048	47.582900
3503.857163	335800.524665	47.587905
3503.832029	335783.065049	47.592909
3504.040978	335770.634393	47.597914
3503.574975	335787.433372	47.602919
3503.639687	335785.030162	47.607924
3503.787935	335778.897009	47.612929
3503.841438	335778.990369	47.617933
3503.856920	335781.253593	47.622938
3503.844041	335779.244506	47.627943
3503.934125	335780.604939	47.632948
3503.809271	335779.428181	47.637953
3504.103604	335768.027768	47.642957
3503.908702	335750.773181	47.647962
3503.806020	335754.429770	47.652967
3503.742188	335755.916363	47.657972
3504.046756	335748.536554	47.662977
3503.748849	335753.802347	47.667981
3503.705538	335763.253775	47.672986
3503.674464	335761.094821	47.677991
3503.635595	335753.107417	47.682996
3503.717430	335759.407836	47.688001
3503.819239	335746.154027	47.693005
3504.037282	335721.833444	47.698010
3503.751582	335714.903341	47.703015
3503.538095	335711.322164	47.708020
3503.777383	335710.877012	47.713025
3503.514035	335716.697402	47.718029
3503.839799	335715.627609	47.723034
3503.900024	335722.542418	47.728039
3503.705751	335723.235003	47.733044
3503.695055	335725.476911	47.738049
3503.999589	335718.148019	47.743053
3503.774352	335720.398384	47.748058
3503.465307	335724.902225	47.753063
3503.357930	335724.333674	47.758068
3503.492614	335731.822227	47.763073
3503.339990	335732.406400	47.768077
3503.583793	335733.309762	47.773082
3503.298626	335733.762144	47.778087
3503.865067	335731.508734	47.783092
3503.577615	335730.383135	47.788097
3503.608974	335731.269167	47.793101
3503.613949	335730.555570	47.798106
3503.428168	335739.800408	47.803111
3503.751374	335735.676164	47.808116
3503.684434	335736.832306	47.813121
3503.689370	335746.887080	47.818125
3503.671669	335737.063416	47.823130
3503.560931	335741.586822	47.828135
3503.726484	335736.952900	47.833140
3503.509469	335755.723640	47.838145
3503.397502	335745.100250	47.843149
3503.893085	335733.668018	47.848154
3503.304558	335749.646289	47.853159
3503.690160	335741.693613	47.858164
3503.592883	335750.389860	47.863169
3503.029265	335750.046174	47.868173
3503.518895	335738.182112	47.873178
3503.562395	335754.060472	47.878183
3503.575169	335750.978130	47.883188
3503.731123	335753.957406	47.888193
3503.803391	335758.375510	47.893197
3504.018858	335751.187987	47.898202
3503.691110	335749.381416	47.903207
3503.724178	335726.261103	47.908212
3503.603478	335723.199859	47.913217
3503.528151	335725.095584	47.918221
3503.695459	335719.061241	47.923226
3503.405792	335733.261187	47.928231
3503.614938	335721.161433	47.933236
3503.732445	335723.179417	47.938241
3503.482710	335725.382740	47.943245
3503.798054	335720.572396	47.948250
3503.793102	335734.269105	47.953255
3503.846995	335730.620205	47.958260
3504.029020	335732.526162	47.963265
3503.851174	335721.556783	47.968269
3503.826709	335728.281322	47.973274
3503.448725	335730.148520	47.978279
3503.775061	335718.132068	47.983284
3503.876351	335730.233641	47.988289
3503.580427	335732.495180	47.993293
3503.916851	335726.612304	47.998298
3503.716771	335715.315496	48.003303
3503.945657	335703.543561	48.008308
3503.649508	335697.327908	48.013313
3503.602439	335696.724366	48.018317
3503.839901	335695.897645	48.023322
3503.746885	335713.885081	48.028327
3503.827064	335699.387281	48.033332
3503.889327	335700.064771	48.038337
3503.644170	335704.151200	48.043341
3503.810269	335697.429703	48.048346
3503.643250	335693.993922	48.053351
3503.676780	335701.040240	48.058356
3503.638087	335701.606403	48.063361
3503.904852	335701.105993	48.068365
3503.808871	335687.679782	48.073370
3503.685811	335679.374736	48.078375
3503.678442	335676.575603	48.083380
3503.630550	335674.699333	48.088385
3503.376892	335679.067136	48.093389
3503.585971	335667.069212	48.098394
3503.686475	335677.210718	48.103399
3504.125805	335673.526342	48.108404
3503.628134	335682.871406	48.113409
3503.740282	335682.930038	48.118413
3504.172102	335685.585680	48.123418
3503.742990	335682.394988	48.128423
3504.076860	335685.422514	48.133428
3503.997737	335675.430350	48.138433
3503.921681	335659.531639	48.143437
3504.082989	335643.060801	48.148442
3503.581622	335647.925993	48.153447
3503.887567	335640.978727	48.158452
3503.800466	335647.484062	48.163457
3503.988422	335645.443223	48.168461
3503.749927	335640.694966	48.173466
3503.527378	335648.952800	48.178471
3503.777817	335649.880571	48.183476
3503.625731	335642.089253	48.188481
3503.671032	335625.000320	48.193485
3503.509056	335608.886065	48.198490
3503.541452	335618.911060	48.203495
3503.439729	335608.515145	48.208500
3503.663218	335630.118403	48.213505
3503.495215	335639.513187	48.218509
3503.600294	335637.052677	48.223514
3503.639490	335647.483908	48.228519
3503.685232	335634.137111	48.233524
3503.890006	335616.692024	48.238529
3503.689962	335619.829411	48.243533
3503.957224	335614.797545	48.248538
3503.707861	335623.365107	48.253543
3503.657526	335613.852069	48.258548
3503.719062	335621.301283	48.263553
3503.967448	335618.410804	48.268557
3504.090291	335611.085164	48.273562
3503.782269	335621.596744	48.278567
3503.896602	335615.825338	48.283572
3503.968021	335590.662343	48.288577
3503.795703	335581.397699	48.293581
3503.920757	335586.469357	48.298586
3503.706436	335590.449089	48.303591
3503.773321	335581.604861	48.308596
3503.857484	335583.118977	48.313601
3503.659765	335596.591615	48.318605
3503.881167	335582.300581	48.323610
3503.648492	335590.152708	48.328615
3503.641496	335593.717808	48.333620
3503.656777	335591.246035	48.338625
3503.503106	335599.085671	48.343629
3503.531564	335586.097997	48.348634
3503.498642	335586.739621	48.353639
3503.587398	335597.672168	48.358644
3503.761164	335600.750464	48.363649
3503.713399	335597.423113	48.368653
3503.958784	335580.811684	48.373658
3503.803055	335580.428976	48.378663
3503.472290	335567.447170	48.383668
3503.623020	335560.702632	48.388673
3503.682712	335570.316004	48.393677
3503.564411	335566.770687	48.398682
3503.662639	335566.500576	48.403687
3503.713814	335568.859995	48.408692
3503.754468	335570.151874	48.413697
3503.541890	335582.201261	48.418701
3503.727204	335572.192737	48.423706
3503.481342	335574.828225	48.428711
3503.649695	335571.619452	48.433716
3504.010843	335581.821599	48.438721
3503.716944	335582.275362	48.443725
3503.712851	335579.552079	48.448730
3503.725188	335582.172208	48.453735
3503.654155	335576.302815	48.458740
3503.616581	335583.360385	48.463745
3503.588678	335584.586730	48.468749
3504.066792	335576.313924	48.473754
3503.587889	335564.781138	48.478759
3503.610023	335552.558174	48.483764
3503.698857	335539.433661	48.488769
3503.562800	335552.081930	48.493773
3503.559212	335543.554324	48.498778
3503.282051	335543.216268	48.503783
3503.559721	335560.839659	48.508788
3503.970573	335567.546315	48.513793
3503.930537	335557.547955	48.518797
3503.952225	335544.739544	48.523802
3503.854167	335548.319042	48.528807
3503.605915	335545.125210	48.533812
3503.609848	335543.469859	48.538817
3503.746549	335545.382986	48.543821
3503.814689	335545.346746	48.548826
3503.994239	335549.111475	48.553831
3503.584873	335540.571642	48.558836
3503.873989	335555.342018	48.563841
3503.227625	335552.491149	48.568845
3503.699740	335548.266983	48.573850
3503.539042	335552.263698	48.578855
3503.472241	335557.620259	48.583860
3503.626338	335564.672989	48.588865
3503.474189	335561.387594	48.593869
3503.552522	335559.134967	48.598874
3503.525601	335560.132042	48.603879
3503.743477	335558.111928	48.608884
3503.807816	335556.905258	48.613889
3503.677351	335551.630773	48.618893
3503.737262	335523.745652	48.623898
3503.957409	335535.293870	48.628903
3503.836945	335524.315388	48.633908
3503.749341	335526.544003	48.638913
3503.764422	335519.337217	48.643917
3503.871252	335521.153238	48.648922
3503.665369	335531.877800	48.653927
3504.060031	335532.248174	48.658932
3504.168446	335528.514272	48.663937
3503.778425	335517.120171	48.668941
3504.027548	335501.144562	48.673946
3503.730869	335494.470744	48.678951
3503.704327	335493.634840	48.683956
3503.854196	335491.345445	48.688961
3503.760157	335493.244134	48.693965
3503.822976	335483.000389	48.698970
3503.531205	335498.499035	48.703975
3503.723903	335491.162340	48.708980
3504.122975	335493.670423	48.713985
3503.931436	335493.369747	48.718989
3503.850249	335468.867261	48.723994
3503.679984	335468.461393	48.728999
3503.619609	335472.900484	48.734004
3503.308566	335472.873270	48.739009
3503.708779	335473.650082	48.744013
3503.839719	335469.174357	48.749018
3503.545206	335476.858071	48.754023
3503.587591	335470.487053	48.759028
3503.534425	335466.524118	48.764033
3503.670260	335476.049096	48.769037
3503.683143	335471.541119	48.774042
3503.564530	335477.287734	48.779047
3503.907094	335478.480975	48.784052
3503.778648	335487.156725	48.789057
3503.702695	335488.110638	48.794061
3503.901113	335480.925781	48.799066
3503.619472	335471.627489	48.804071
3503.817266	335477.985975	48.809076
3503.672910	335485.569580	48.814081
3503.689619	335496.055303	48.819085
3503.907811	335484.106820	48.824090
3503.643105	335474.347622	48.829095
3503.819797	335455.354041	48.834100
3503.933697	335449.608147	48.839105
3503.642810	335447.388425	48.844109
3503.923877	335447.267611	48.849114
3503.728834	335453.535456	48.854119
3503.577169	335442.587350	48.859124
3504.198497	335432.764453	48.864129
3503.796503	335450.851716	48.869133
3503.914527	335442.635816	48.874138
3503.644788	335439.241718	48.879143
3503.490233	335425.111911	48.884148
3503.494112	335421.649101	48.889153
3503.515910	335437.021821	48.894157
3503.594327	335437.162157	48.899162
3503.775253	335451.440514	48.904167
3503.586775	335426.344000	48.909172
3503.662492	335424.906414	48.914177
3503.645073	335412.766048	48.919181
3503.745796	335420.056346	48.924186
3503.816703	335421.496189	48.929191
3503.935684	335421.910143	48.934196
3504.078463	335425.324290	48.939201
3503.577111	335413.158595	48.944205
3504.181999	335416.907009	48.949210
3503.690944	335419.377605	48.954215
3503.842417	335415.916920	48.959220
3503.587682	335404.908730	48.964225
3503.746703	335399.461186	48.969229
3503.523783	335391.273720	48.974234
3503.598411	335395.895133	48.979239
3503.541490	335381.240738	48.984244
3503.616303	335383.061823	48.989249
3503.430350	335390.677471	48.994253
3503.561807	335381.008377	48.999258
3503.586553	335398.213562	49.004263
3503.629038	335399.250583	49.009268
3503.636143	335388.379199	49.014273
3503.512529	335383.434563	49.019277
3504.022322	335388.267215	49.024282
3503.612303	335400.246017	49.029287
3503.846469	335382.363450	49.034292
3503.790844	335390.314898	49.039297
3503.450463	335397.573099	49.044301
3503.967148	335398.891559	49.049306
3503.341234	335404.743832	49.054311
3503.452899	335397.343565	49.059316
3503.606283	335396.657418	49.064321
3503.323645	335404.619293	49.069325
3503.649337	335399.247231	49.074330
3503.486682	335404.949900	49.079335
3503.699732	335400.792135	49.084340
3503.719117	335399.032508	49.089345
3503.613977	335407.042696	49.094349
3503.838571	335395.475044	49.099354
3503.871500	335402.801518	49.104359
3503.635520	335407.472031	49.109364
3503.540861	335405.272202	49.114369
3503.620929	335402.281035	49.119373
3503.787408	335405.691437	49.124378
3503.430558	335415.854366	49.129383
3503.797832	335402.914926	49.134388
3503.669100	335412.023504	49.139393
3503.411448	335416.773814	49.144397
3503.824308	335416.657624	49.149402
3503.324905	335416.660187	49.154407
3503.683562	335418.665516	49.159412
3503.877365	335412.805159	49.164417
3503.879773	335412.830224	49.169421
3503.892609	335388.236475	49.174426
3503.636607	335392.375551	49.179431
3503.673865	335379.284618	49.184436
3503.756113	335376.140362	49.189441
3503.610355	335379.549209	49.194445
3503.615410	335371.783933	49.199450
3503.632475	335378.578314	49.204455
3503.433797	335381.537295	49.209460
3503.505888	335384.962618	49.214465
3503.660053	335384.352720	49.219469
3503.601006	335379.219676	49.224474
3503.416797	335384.823925	49.229479
3503.714151	335381.442007	49.234484
3503.904479	335380.215418	49.239489
3503.598462	335389.581139	49.244493
3504.075900	335380.442870	49.249498
3503.458973	335382.755164	49.254503
3503.665530	335382.136984	49.259508
3503.860821	335392.289006	49.264513
3503.854804	335391.220741	49.269517
3503.862223	335393.103394	49.274522
3503.873957	335384.038744	49.279527
3503.992814	335365.741627	49.284532
3504.097660	335351.036196	49.289537
3503.699288	335359.856462	49.294541
3503.924237	335354.678522	49.299546
3503.951791	335357.550827	49.304551
3503.841527	335363.245218	49.309556
3503.800012	335358.007571	49.314561
3503.637437	335356.658568	49.319565
3503.643497	335345.481855	49.324570
3503.536751	335335.137606	49.329575
3503.667724	335328.090681	49.334580
3503.627415	335316.615807	49.339585
3503.424515	335324.081398	49.344589
3503.622016	335322.064497	49.349594
3503.591755	335330.011942	49.354599
3503.567796	335328.411910	49.359604
3503.697974	335328.238577	49.364609
3503.507579	335321.166081	49.369613
3503.628980	335317.913804	49.374618
3503.675484	335322.310552	49.379623
3503.368682	335332.236466	49.384628
3503.605165	335328.482308	49.389633
3503.721621	335330.831415	49.394637
3503.776719	335333.546623	49.399642
3503.754969	335332.379016	49.404647
3503.652959	335335.017230	49.409652
3503.709245	335334.040945	49.414657
3503.546473	335337.401569	49.419661
3503.779172	335332.451517	49.424666
3503.489199	335340.185444	49.429671
3503.401226	335340.453912	49.434676
3503.669113	335333.843576	49.439681
3503.455473	335343.092872	49.444685
3503.718449	335344.553269	49.449690
3503.509099	335339.113037	49.454695
3503.770634	335344.646827	49.459700
3503.932582	335344.213898	49.464705
3503.431166	335346.635220	49.469709
3503.889758	335340.223853	49.474714
3503.574988	335347.732583	49.479719
3503.501354	335352.733838	49.484724
3503.642583	335346.525384	49.489729
3503.419707	335354.019586	49.494733
3503.728117	335343.966113	49.499738
3503.169450	335351.869799	49.504743
3503.582382	335343.454526	49.509748
3503.728902	335349.388355	49.514753
3503.751669	335344.395119	49.519757
3503.663380	335347.031164	49.524762
3503.529891	335348.859722	49.529767
3503.389374	335356.926422	49.534772
3503.716036	335355.754653	49.539777
3503.406736	335356.236309	49.544781
3503.585038	335362.521515	49.549786
3503.471697	335363.430426	49.554791
3503.626823	335365.773419	49.559796
3503.920843	335363.664890	49.564801
3503.410788	335364.687427	49.569805
3503.906964	335366.212789	49.574810
3503.722637	335369.474989	49.579815
3503.753179	335358.370781	49.584820
3504.068711	335357.684459	49.589825
3503.618789	335350.118389	49.594829
3503.809477	335327.558542	49.599834
3503.772240	335334.106939	49.604839
3503.884333	335332.358113	49.609844
3503.793164	335330.539590	49.614849
3503.696181	335335.009934	49.619853
3503.768249	335322.091688	49.624858
3503.464181	335333.544607	49.629863
3503.502113	335336.440730	49.634868
3503.611056	335333.164965	49.639873
3503.624313	335337.541511	49.644877
3503.900544	335341.596455	49.649882
3503.980234	335342.958540	49.654887
3503.950726	335337.795366	49.659892
3504.003722	335324.167331	49.664897
3503.642040	335313.303319	49.669901
3503.900356	335297.886269	49.674906
3503.967301	335309.738774	49.679911
3503.762912	335301.191965	49.684916
3503.911155	335300.735746	49.689921
3503.592185	335309.568923	49.694925
3503.857401	335299.445899	49.699930
3503.456266	335306.153653	49.704935
3503.565070	335306.238271	49.709940
3503.631703	335297.775906	49.714945
3503.273656	335307.862668	49.719949
3503.601011	335305.010607	49.724954
3503.714410	335306.952881	49.729959
3503.561689	335307.053384	49.734964
3504.080391	335305.316653	49.739969
3503.558670	335322.124554	49.744973
3503.801987	335316.205446	49.749978
3503.750701	335316.951804	49.754983
3503.824761	335297.236142	49.759988
3503.908073	335281.770382	49.764993
3503.361508	335278.267292	49.769997
3503.645397	335268.828659	49.775002
3503.547352	335267.978599	49.780007
3503.575418	335273.854788	49.785012
3503.475102	335264.476890	49.790017
3503.405344	335274.314426	49.795021
3503.600510	335270.795912	49.800026
3503.503341	335288.147684	49.805031
3503.314870	335279.420155	49.810036
3503.551360	335281.953947	49.815041
3503.258473	335297.885589	49.820045
3503.555102	335310.720077	49.825050
3503.513161	335316.836445	49.830055
3503.532096	335322.688616	49.835060
3503.661546	335331.807306	49.840065
3503.759284	335325.351152	49.845069
3503.773554	335320.002856	49.850074
3503.715207	335302.471996	49.855079
3503.776442	335292.737618	49.860084
3503.527876	335289.391080	49.865089
3503.468988	335290.316841	49.870093
3503.753977	335293.072082	49.875098
3503.763648	335286.502559	49.880103
3503.731749	335293.151945	49.885108
3504.022576	335293.360533	49.890113
3503.827294	335298.100992	49.895117
3503.864679	335283.558955	49.900122
3503.722163	335287.094580	49.905127
3503.768738	335293.273329	49.910132
3504.043787	335285.261704	49.915137
3503.609728	335280.747995	49.920141
3503.896043	335259.445874	49.925146
3503.755687	335258.449759	49.930151
3503.968448	335255.361237	49.935156
3503.699111	335258.916912	49.940161
3503.725968	335256.545125	49.945165
3504.216178	335255.143842	49.950170
3503.580241	335257.280944	49.955175
3503.590689	335256.464648	49.960180
3503.809418	335251.262226	49.965185
3503.728058	335262.298091	49.970189
3503.693558	335252.731586	49.975194
3503.780702	335253.506976	49.980199
3503.817658	335238.354021	49.985204
3503.778004	335225.886193	49.990209
3503.719474	335220.600311	49.995213
3503.628516	335214.683122	50.000218
3503.555905	335230.732702	50.005223
3503.533146	335228.572417	50.010228
3503.737150	335221.743052	50.015233
3503.585902	335227.800335	50.020237
3503.698711	335216.148495	50.025242
3503.712005	335222.357970	50.030247
3503.707068	335216.503555	50.035252
3503.529759	335222.361300	50.040257
3503.409226	335229.126533	50.045261
3503.960180	335229.548573	50.050266
3503.898666	335240.123073	50.055271
3503.678836	335234.811776	50.060276
3503.979123	335225.726948	50.065281
3503.743861	335232.459402	50.070285
3504.015143	335220.706139	50.075290
3503.700465	335202.248396	50.080295
3503.739658	335195.674198	50.085300
3503.442749	335191.240632	50.090305
3503.778264	335196.813653	50.095309
3503.819953	335185.198508	50.100314
3503.793031	335193.756417	50.105319
3503.593647	335190.223898	50.110324
3503.912723	335196.766896	50.115329
3503.861908	335196.800375	50.120333
3504.003465	335193.875851	50.125338
3503.875956	335201.762312	50.130343
3504.171606	335194.663884	50.135348
3503.972522	335173.667584	50.140353
3503.698426	335177.504046	50.145357
3503.581285	335167.161415	50.150362
3503.590229	335169.883926	50.155367
3503.570330	335172.840112	50.160372
3503.936990	335162.090055	50.165377
3503.951632	335175.707408	50.170381
3504.004190	335170.302132	50.175386
3503.826952	335175.421607	50.180391
3503.822978	335157.398425	50.185396
3503.735712	335149.036742	50.190401
3503.603975	335145.060752	50.195405
3503.575380	335132.845731	50.200410
3503.693756	335134.176247	50.205415
3503.463882	335145.973872	50.210420
3503.520211	335138.633239	50.215425
3503.545977	335135.396071	50.220429
3503.970413	335130.339323	50.225434
3503.725477	335141.019206	50.230439
3503.548510	335135.650211	50.235444
3503.852689	335131.376194	50.240449
3503.709262	335139.443380	50.245453
3503.526675	335133.769785	50.250458
3503.530245	335146.523344	50.255463
3503.415611	335136.791288	50.260468
3503.753230	335143.585934	50.265473
3503.507775	335147.494242	50.270477
3503.424864	335141.983092	50.275482
3503.816550	335144.339612	50.280487
3503.794250	335143.375747	50.285492
3503.941287	335144.116212	50.290497
3503.531770	335143.366303	50.295501
3503.504337	335141.359497	50.300506
3503.724761	335148.707274	50.305511
3503.802174	335149.738776	50.310516
3503.957613	335140.269516	50.315521
3503.703148	335145.859434	50.320525
3503.669889	335117.403356	50.325530
3503.665309	335115.418395	50.330535
3504.246535	335105.881822	50.335540
3504.265335	335109.417413	50.340545
3503.609679	335115.605358	50.345549
3503.817690	335109.004465	50.350554
3503.905145	335115.609543	50.355559
3503.626050	335101.193868	50.360564
3503.692205	335111.722749	50.365569
3503.549421	335113.145464	50.370573
3503.634663	335112.393714	50.375578
3503.740989	335112.453267	50.380583
3503.564350	335105.327660	50.385588
3503.770218	335098.192500	50.390593
3503.297890	335096.230565	50.395597
3503.849297	335095.965186	50.400602
3503.566008	335096.722764	50.405607
3503.414148	335092.368091	50.410612
3503.490565	335095.538171	50.415617
3503.681613	335110.858751	50.420621
3503.601436	335109.394888	50.425626
3503.512178	335102.790071	50.430631
3503.528141	335100.547289	50.435636
3503.503102	335096.172568	50.440641
3503.424780	335105.756909	50.445645
3503.754671	335109.141493	50.450650
3503.538175	335115.158186	50.455655
3503.584452	335123.679075	50.460660
3503.767434	335119.093271	50.465665
3503.687328	335116.891132	50.470669
3503.935418	335096.180523	50.475674
3503.918249	335101.300157	50.480679
3503.566092	335093.642232	50.485684
3503.902015	335092.927227	50.490689
3503.778560	335096.561678	50.495693
3503.940482	335097.427078	50.500698
3503.674845	335107.346517	50.505703
3503.742413	335105.655639	50.510708
3503.707152	335100.391527	50.515713
3503.725783	335111.742556	50.520717
3503.544805	335106.781510	50.525722
3503.485268	335097.982662	50.530727
3503.541255	335072.261854	50.535732
3503.674052	335056.151785	50.540737
3503.160987	335027.720604	50.545741
3503.362358	334984.563921	50.550746
3503.016252	334940.653660	50.555751
3502.879246	334889.225829	50.560756
3502.733436	334824.052318	50.565761
3502.425007	334774.713555	50.570765
3502.058988	334694.834846	50.575770
3501.933798	334620.467719	50.580775
3501.296731	334538.035007	50.585780
3501.145707	334442.338322	50.590785
3500.597575	334349.886486	50.595789
3500.722152	334242.919137	50.600794
3500.329493	334143.568874	50.605799
3499.882576	334023.122565	50.610804
3499.605539	333912.374074	50.615809
3498.505213	333787.931946	50.620813
3498.915575	333658.031915	50.625818
3498.049563	333535.741678	50.630823
3497.887723	333412.347050	50.635828
3497.549973	333259.423236	50.640833
3496.701558	333123.713116	50.645837
3496.244917	332982.747343	50.650842
3495.818397	332834.571862	50.655847
3495.214540	332681.714332	50.660852
3494.527200	332540.707781	50.665857
3493.934797	332394.441525	50.670861
3493.774231	332226.925314	50.675866
3492.915756	332075.634250	50.680871
3492.240381	331923.448334	50.685876
3491.578235	331758.785309	50.690881
3490.849235	331606.607206	50.695885
3490.324433	331439.197673	50.700890
3489.966467	331277.260471	50.705895
3489.446074	331117.665338	50.710900
3488.636607	330937.519346	50.715905
3487.888453	330782.898513	50.720909
3487.311530	330615.749936	50.725914
3487.084597	330452.440883	50.730919
3486.096116	330283.421735	50.735924
3485.560784	330110.588073	50.740929
3484.934903	329947.722874	50.745933
3484.074960	329780.489873	50.750938
3483.412588	329612.461489	50.755943
3482.867646	329436.572682	50.760948
3482.330118	329263.941102	50.765953
3481.410531	329108.376462	50.770957
3480.937176	328936.777835	50.775962
3480.445159	328761.337375	50.780967
3479.758511	328601.152153	50.785972
3479.130155	328423.823004	50.790977
3478.794345	328240.973351	50.795981
3477.881644	328063.051834	50.800986
3477.177184	327898.387047	50.805991
3476.491361	327718.086567	50.810996
3476.022901	327537.216649	50.816001
3475.091249	327378.595245	50.821005
3474.468479	327193.471646	50.826010
3473.869790	327020.361003	50.831015
3473.050789	326846.011803	50.836020
3472.698739	326663.237429	50.841025
3471.805121	326503.080648	50.846029
3471.584189	326313.104935	50.851034
3470.856718	326139.910906	50.856039
3469.818839	325955.257435	50.861044
3469.407154	325768.391319	50.866049
3468.575195	325604.276623	50.871053
3468.057045	325415.618828	50.876058
3467.195900	325234.653042	50.881063
3466.538944	325063.609740	50.886068
3466.284674	324880.714058	50.891073
3465.288667	324713.288150	50.896077
3464.782136	324525.313929	50.901082
3463.678519	324347.770846	50.906087
3463.512727	324165.597975	50.911092
3463.375144	323989.174460	50.916097
3462.043819	323816.605709	50.921101
3461.165897	323625.862006	50.926106
3460.249951	323445.512083	50.931111
3459.591906	323279.328421	50.936116
3459.037129	323099.633586	50.941121
3458.484702	322935.902314	50.946125
3457.806870	322748.078547	50.951130
3457.114034	322576.068352	50.956135
3456.453822	322408.788511	50.961140
3456.374594	322223.313283	50.966145
3455.312249	322051.997015	50.971149
3454.564640	321859.726576	50.976154
3454.029003	321678.778161	50.981159
3453.172302	321505.722382	50.986164
3452.615793	321317.367137	50.991169
3451.579739	321145.306566	50.996173
3451.084336	320968.908037	51.001178
3450.562507	320807.994255	51.006183
3449.347217	320626.692851	51.011188
3448.970911	320445.538524	51.016193
3447.966625	320290.250846	51.021197
3447.610319	320105.247893	51.026202
3447.154831	319936.403330	51.031207
3446.252146	319763.835276	51.036212
3445.754225	319587.510862	51.041217
3444.899646	319419.517788	51.046221
3444.643811	319242.237798	51.051226
3444.103567	319062.048788	51.056231
3443.002682	318886.327632	51.061236
3442.555639	318699.681166	51.066241
3441.626154	318532.513153	51.071245
3441.188350	318358.952360	51.076250
3440.306898	318183.246136	51.081255
3439.900571	318011.742219	51.086260
3438.894778	317827.372191	51.091265
3438.079861	317664.844254	51.096269
3437.805069	317486.723723	51.101274
3437.072556	317318.351167	51.106279
3435.954822	317141.814672	51.111284
3435.881438	316962.642824	51.116289
3434.903583	316807.141568	51.121293
3434.496927	316622.318061	51.126298
3433.749590	316444.957866	51.131303
3433.102762	316267.683319	51.136308
3432.585634	316087.816160	51.141313
3431.714522	315919.208516	51.146317
3430.937614	315737.573912	51.151322
3430.237067	315561.758034	51.156327
3429.748436	315392.248750	51.161332
3429.292019	315207.303207	51.166337
3427.974364	315039.146668	51.171341
3427.460918	314870.735384	51.176346
3426.777139	314701.026650	51.181351
3426.123815	314533.655483	51.186356
3425.279573	314357.147298	51.191361
3424.494663	314193.997910	51.196365
3424.333214	314022.372104	51.201370
3423.437296	313854.299768	51.206375
3422.840431	313688.293386	51.211380
3422.064748	313506.782030	51.216385
3421.285060	313346.457017	51.221389
3420.870121	313181.821608	51.226394
3420.273554	313006.570700	51.231399
3419.580525	312828.279074	51.236404
3419.011803	312658.065093	51.241409
3418.172049	312491.204045	51.246413
3417.566590	312311.191638	51.251418
3416.607381	312147.812092	51.256423
3416.017242	311981.114525	51.261428
3415.529458	311814.196812	51.266433
3414.614314	311648.288606	51.271437
3414.195025	311473.287361	51.276442
3413.514738	311303.445466	51.281447
3412.805130	311139.006420	51.286452
3412.309079	310959.458389	51.291457
3411.412531	310790.592118	51.296461
3410.882864	310610.997933	51.301466
3410.227227	310446.014614	51.306471
3409.399827	310285.081638	51.311476
3408.995955	310105.008424	51.316481
3408.018928	309940.406257	51.321485
3407.441001	309771.640931	51.326490
3406.782947	309605.943812	51.331495
3406.365157	309430.608233	51.336500
3405.538990	309264.071421	51.341505
3404.485735	309100.447823	51.346509
3404.070439	308930.789801	51.351514
3403.174624	308761.538568	51.356519
3402.531046	308594.717325	51.361524
3402.095551	308424.832616	51.366529
3401.530523	308266.783950	51.371533
3400.883949	308086.262291	51.376538
3400.455875	307913.956529	51.381543
3399.539228	307749.876644	51.386548
3398.850944	307577.178662	51.391553
3398.031114	307417.488522	51.396557
3397.510479	307239.415875	51.401562
3396.753859	307066.422429	51.406567
3395.819739	306913.752699	51.411572
3395.664107	306737.811668	51.416577
3394.410785	306577.221356	51.421581
3393.731054	306402.941606	51.426586
3393.141335	306241.456526	51.431591
3392.560949	306083.458549	51.436596
3391.891026	305912.588985	51.441601
3390.911613	305753.074853	51.446605
3390.664490	305579.820646	51.451610
3390.293204	305426.016126	51.456615
3389.633254	305263.344100	51.461620
3389.080078	305084.917203	51.466625
3388.390234	304916.570648	51.471629
3387.660420	304738.298567	51.476634
3387.176356	304576.642021	51.481639
3386.303945	304402.339259	51.486644
3385.527135	304224.175823	51.491649
3384.513481	304064.385046	51.496653
3384.061314	303899.106534	51.501658
3383.578259	303740.351994	51.506663
3382.823557	303565.851343	51.511668
3382.247206	303393.639685	51.516673
3381.134552	303235.366146	51.521677
3380.782239	303064.824901	51.526682
3380.410614	302892.707618	51.531687
3379.554715	302728.077352	51.536692
3379.161318	302554.969947	51.541697
3378.273455	302399.766847	51.546701
3377.670193	302216.760441	51.551706
3376.854388	302046.164009	51.556711
3376.097364	301885.948322	51.561716
3375.564017	301714.084480	51.566721
3374.558708	301549.960437	51.571725
3373.828165	301383.628137	51.576730
3373.184925	301217.179992	51.581735
3372.369987	301054.757045	51.586740
3372.294248	300889.364805	51.591745
3371.489769	300735.649393	51.596749
3370.796832	300564.599009	51.601754
3370.350008	300403.899852	51.606759
3369.524920	300231.087365	51.611764
3368.799406	300060.958405	51.616769
3368.269167	299889.474130	51.621773
3367.692198	299719.576000	51.626778
3366.933277	299554.774327	51.631783
3366.087360	299390.903051	51.636788
3365.906304	299217.707550	51.641793
3364.719743	299056.487424	51.646797
3364.141775	298889.389966	51.651802
3363.159309	298725.412323	51.656807
3362.520436	298552.441362	51.661812
3362.189132	298385.406288	51.666817
3361.210695	298229.194919	51.671821
3360.508847	298067.336974	51.676826
3360.203369	297904.601265	51.681831
3359.258175	297748.384226	51.686836
3358.482452	297574.517168	51.691841
3357.964534	297423.452999	51.696845
3357.282056	297258.076849	51.701850
3356.856622	297099.663317	51.706855
3356.121962	296926.527708	51.711860
3355.528893	296760.984185	51.716865
3354.611745	296600.712510	51.721869
3354.266243	296430.061617	51.726874
3353.586003	296257.553481	51.731879
3352.631167	296102.813713	51.736884
3352.449257	295930.328355	51.741889
3351.616328	295765.815146	51.746893
3350.604910	295598.044768	51.751898
3350.052524	295434.454678	51.756903
3349.228314	295268.080586	51.761908
3348.952689	295107.986409	51.766913
3348.067347	294946.791573	51.771917
3347.495965	294777.397444	51.776922
3346.721705	294620.310488	51.781927
3345.934292	294454.846760	51.786932
3345.781771	294286.302826	51.791937
3344.885744	294118.054615	51.796941
3344.010944	293955.405735	51.801946
3343.460295	293788.605228	51.806951
3342.383618	293626.701123	51.811956
3341.915895	293465.133544	51.816961
3340.925534	293321.577566	51.821965
3340.311945	293165.228197	51.826970
3339.817091	293003.257107	51.831975
3338.968269	292847.861557	51.836980
3338.616057	292684.314174	51.841985
3337.967965	292525.524960	51.846989
3337.256443	292368.477465	51.851994
3336.767467	292210.834387	51.856999
3335.987255	292044.629235	51.862004
3335.392085	291872.995583	51.867009
3334.636488	291727.389590	51.872013
3334.193701	291550.739974	51.877018
3333.455611	291395.606140	51.882023
3332.502156	291240.277065	51.887028
3332.106119	291065.784473	51.892033
3331.334242	290914.679586	51.897037
3330.738800	290753.563381	51.902042
3329.971396	290588.144768	51.907047
3329.507813	290431.082349	51.912052
3328.621708	290271.896439	51.917057
3327.760694	290114.336406	51.922061
3327.395087	289954.787853	51.927066
3326.838567	289791.347369	51.932071
3325.847267	289635.564952	51.937076
3325.240484	289467.140549	51.942081
3324.253977	289309.778198	51.947085
3323.739449	289150.049016	51.952090
3323.333647	288996.694980	51.957095
3322.846359	288835.331383	51.962100
3322.592554	288666.825241	51.967105
3321.375110	288517.190301	51.972109
3320.993945	288351.683875	51.977114
3320.432595	288183.659071	51.982119
3319.400083	288018.688442	51.987124
3319.015059	287852.749418	51.992129
3317.790626	287703.064275	51.997133
3317.187138	287541.667474	52.002138
3316.747328	287378.232741	52.007143
3315.879410	287218.685836	52.012148
3315.475831	287063.267638	52.017153
3314.460180	286913.701943	52.022157
3314.033890	286747.412366	52.027162
3313.534856	286585.667526	52.032167
3312.508397	286427.342344	52.037172
3312.123851	286277.702046	52.042177
3311.752387	286110.130114	52.047181
3310.961876	285947.208637	52.052186
3310.187857	285788.868737	52.057191
3309.762117	285620.515672	52.062196
3309.275535	285457.545927	52.067201
3308.113243	285300.031290	52.072205
3307.314041	285134.589522	52.077210
3306.832437	284973.528912	52.082215
3306.092924	284808.867091	52.087220
3305.480108	284661.070547	52.092225
3304.685484	284500.670509	52.097229
3304.094286	284337.742362	52.102234
3303.360720	284179.191731	52.107239
3302.700842	284024.729769	52.112244
3302.291993	283857.875987	52.117249
3301.463142	283698.423416	52.122253
3300.830804	283536.214617	52.127258
3300.408698	283373.106597	52.132263
3299.368836	283212.617587	52.137268
3299.202703	283059.809080	52.142273
3298.032194	282895.393065	52.147277
3297.301727	282732.206284	52.152282
3296.709954	282579.643246	52.157287
3295.894278	282424.186733	52.162292
3295.538185	282256.687409	52.167297
3294.478783	282098.824410	52.172301
3293.874479	281951.433253	52.177306
3293.603379	281792.273956	52.182311
3292.611542	281638.984448	52.187316
3292.288175	281469.085726	52.192321
3291.370067	281321.081889	52.197325
3290.447263	281156.931865	52.202330
3289.872804	281011.522315	52.207335
3289.014849	280860.452676	52.212340
3288.568373	280700.378547	52.217345
3287.813697	280550.693272	52.222349
3286.940588	280392.418408	52.227354
3286.502747	280237.512895	52.232359
3285.776155	280088.689020	52.237364
3285.249811	279934.561502	52.242369
3284.444561	279789.213714	52.247373
3283.543272	279630.281001	52.252378
3283.183081	279475.974321	52.257383
3282.234469	279332.788486	52.262388
3282.001245	279175.405479	52.267393
3281.291635	279028.565296	52.272397
3280.897437	278867.311050	52.277402
3280.166398	278716.475687	52.282407
3279.279321	278563.729391	52.287412
3278.637449	278407.353255	52.292417
3278.174239	278254.463478	52.297421
3277.569546	278090.186233	52.302426
3277.027543	277930.916325	52.307431
3276.049044	277779.636112	52.312436
3275.674278	277616.010101	52.317441
3274.932437	277458.325335	52.322445
3274.328834	277294.939243	52.327450
3273.605685	277146.674801	52.332455
3272.407896	276988.756504	52.337460
3272.114403	276836.578360	52.342465
3271.279100	276688.484447	52.347469
3271.033337	276516.815422	52.352474
3270.092287	276364.204850	52.357479
3269.297015	276213.328535	52.362484
3268.743512	276048.279018	52.367489
3268.373042	275894.533981	52.372493
3267.699932	275750.998702	52.377498
3266.671182	275590.455852	52.382503
3265.920060	275433.714817	52.387508
3265.306141	275281.001554	52.392513
3264.563674	275128.767059	52.397517
3264.076118	274970.099678	52.402522
3263.568693	274813.243701	52.407527
3262.669457	274666.535186	52.412532
3261.915372	274509.921983	52.417537
3261.321546	274353.207031	52.422541
3260.775928	274205.194650	52.427546
3260.221046	274053.618168	52.432551
3259.191372	273892.056786	52.437556
3258.858512	273735.453401	52.442561
3257.925315	273582.408689	52.447565
3257.364311	273431.953826	52.452570
3256.840968	273276.628559	52.457575
3256.067426	273128.805115	52.462580
3255.572588	272968.025135	52.467585
3254.743150	272817.510916	52.472589
3253.837425	272662.500879	52.477594
3253.299799	272509.979468	52.482599
3252.625634	272370.061044	52.487604
3251.991540	272202.757813	52.492609
3251.220983	272061.148292	52.497613
3250.646688	271920.195390	52.502618
3250.385260	271766.688056	52.507623
3249.715548	271606.216065	52.512628
3249.170293	271441.394795	52.517633
3248.232431	271283.588513	52.522637
3247.663689	271137.388364	52.527642
3246.979426	270980.127790	52.532647
3246.195103	270821.074821	52.537652
3245.521804	270659.788576	52.542657
3244.861507	270518.416527	52.547661
3244.123280	270361.215543	52.552666
3243.622011	270207.746416	52.557671
3242.766964	270060.955040	52.562676
3242.359901	269895.526445	52.567681
3241.439133	269746.478851	52.572685
3240.749632	269580.865793	52.577690
3240.386086	269436.900183	52.582695
3239.379171	269285.752453	52.587700
3239.055562	269118.375257	52.592705
3238.188144	268972.146378	52.597709
3237.473091	268817.616250	52.602714
3237.195890	268672.974982	52.607719
3236.043038	268507.868465	52.612724
3235.484746	268357.872475	52.617729
3234.882290	268211.932959	52.622733
3233.944956	268056.011979	52.627738
3233.574753	267895.136902	52.632743
3232.682157	267757.571510	52.637748
3232.175563	267602.193763	52.642753
3231.031733	267457.435228	52.647757
3230.474879	267307.184627	52.652762
3229.993365	267164.740883	52.657767
3229.281403	267013.776333	52.662772
3228.388331	266855.607525	52.667777
3227.983743	266722.345749	52.672781
3227.453678	266571.760058	52.677786
3226.774597	266424.432443	52.682791
3225.894447	266271.228081	52.687796
3225.655541	266125.817447	52.692801
3224.756758	265976.971184	52.697805
3224.158306	265819.392843	52.702810
3223.413185	265662.780083	52.707815
3222.745617	265518.787279	52.712820
3221.954544	265374.610321	52.717825
3220.982241	265232.856082	52.722829
3220.630988	265077.913071	52.727834
3220.219247	264934.160159	52.732839
3219.370078	264793.176111	52.737844
3219.156071	264633.321707	52.742849
3218.260789	264492.446940	52.747853
3217.483549	264331.128220	52.752858
3217.000668	264176.384681	52.757863
3216.332994	264023.809753	52.762868
3215.491314	263863.978582	52.767873
3214.833289	263717.540040	52.772877
3214.278450	263570.015585	52.777882
3213.807765	263426.985704	52.782887
3212.625140	263276.530007	52.787892
3211.895932	263122.946501	52.792897
3211.248014	262978.824265	52.797901
3210.589136	262828.056709	52.802906
3210.018257	262682.241538	52.807911
3209.379929	262535.545730	52.812916
3208.912111	262389.459712	52.817921
3207.736205	262252.781544	52.822925
3207.419317	262097.376028	52.827930
3207.027539	261947.967375	52.832935
3206.101257	261813.974971	52.837940
3205.579662	261651.343749	52.842945
3204.879462	261506.670185	52.847949
3204.345968	261352.649120	52.852954
3203.818295	261199.238443	52.857959
3202.925300	261050.673578	52.862964
3202.401695	260903.680288	52.867969
3201.379414	260756.816902	52.872973
3200.694331	260595.561940	52.877978
3200.148296	260449.260069	52.882983
3199.083966	260322.141022	52.887988
3198.627492	260172.132322	52.892993
3198.119481	260026.053877	52.897997
3197.169012	259877.906233	52.903002
3196.718516	259728.278856	52.908007
3195.875874	259600.284658	52.913012
3195.100560	259440.674606	52.918017
3194.457934	259303.760729	52.923021
3194.136007	259162.339370	52.928026
3193.572764	259008.222501	52.933031
3192.816414	258877.719203	52.938036
3192.410483	258724.698197	52.943041
3191.669653	258575.091979	52.948045
3190.727440	258420.169546	52.953050
3190.246112	258270.165920	52.958055
3189.359953	258133.393104	52.963060
3188.731471	257989.550592	52.968065
3187.946432	257847.260982	52.973069
3187.499849	257704.332165	52.978074
3186.704399	257542.638239	52.983079
3185.721187	257407.791265	52.988084
3185.591433	257266.824520	52.993089
3185.001296	257127.127666	52.998093
3184.045920	256980.918119	53.003098
3183.595460	256829.433458	53.008103
3182.656463	256686.073855	53.013108
3182.388392	256537.260074	53.018113
3181.230911	256401.957414	53.023117
3180.718081	256240.678149	53.028122
3180.195605	256097.787855	53.033127
3179.194492	255961.238314	53.038132
3178.844027	255821.657197	53.043137
3178.103597	255683.513099	53.048141
3177.311554	255534.349989	53.053146
3176.480115	255396.500623	53.058151
3175.938191	255246.661475	53.063156
3175.443662	255107.332846	53.068161
3174.954493	254968.054400	53.073165
3174.018987	254822.021502	53.078170
3173.819107	254686.797680	53.083175
3172.462407	254532.376583	53.088180
3172.746189	254381.286907	53.093185
3171.917526	254231.111897	53.098189
3170.913028	254089.114249	53.103194
3170.285150	253944.510427	53.108199
3169.567226	253803.766467	53.113204
3169.038058	253654.130270	53.118209
3167.867979	253516.743294	53.123213
3167.435409	253374.069964	53.128218
3166.845228	253225.156840	53.133223
3165.944966	253089.280972	53.138228
3165.454755	252946.617096	53.143233
3164.672279	252800.052224	53.148237
3164.058206	252660.973521	53.153242
3163.449028	252520.136947	53.158247
3162.726420	252380.897368	53.163252
3162.458649	252234.226062	53.168257
3161.568597	252097.381604	53.173261
3160.535309	251952.639789	53.178266
3159.989567	251808.075623	53.183271
3159.495740	251668.418420	53.188276
3158.866258	251518.799893	53.193281
3158.241954	251378.934372	53.198285
3157.781631	251242.557406	53.203290
3157.009326	251095.737706	53.208295
3156.153622	250958.430335	53.213300
3155.880304	250814.536980	53.218305
3155.141429	250670.488215	53.223309
3154.408542	250517.372579	53.228314
3153.688781	250379.560322	53.233319
3152.848197	250238.227472	53.238324
3152.360760	250086.423128	53.243329
3151.906293	249933.671457	53.248333
3150.955056	249795.412467	53.253338
3150.258638	249646.137308	53.258343
3149.584047	249514.685226	53.263348
3149.094175	249358.425369	53.268353
3148.488096	249215.528355	53.273357
3147.900462	249078.613112	53.278362
3147.071623	248924.571953	53.283367
3146.549447	248785.863982	53.288372
3145.952660	248634.562211	53.293377
3145.432702	248483.706824	53.298381
3144.235187	248339.860103	53.303386
3143.339394	248184.276863	53.308391
3142.593317	248041.836030	53.313396
3142.299331	247911.725744	53.318401
3141.427094	247778.269161	53.323405
3140.715586	247644.405279	53.328410
3140.306146	247490.095514	53.333415
3139.594902	247353.328742	53.338420
3138.933791	247214.109443	53.343425
3138.175623	247080.609988	53.348429
3137.341735	246938.718914	53.353434
3136.749260	246792.893516	53.358439
3135.987894	246664.258926	53.363444
3135.276463	246510.227195	53.368449
3134.519438	246386.965447	53.373453
3134.205213	246254.262363	53.378458
3133.573626	246112.441977	53.383463
3132.787723	245977.674674	53.388468
3132.406758	245828.633609	53.393473
3131.269170	245692.801747	53.398477
3130.618151	245554.066350	53.403482
3130.077217	245416.255902	53.408487
3129.120619	245292.033561	53.413492
3129.019619	245142.821621	53.418497
3128.064032	245013.939191	53.423501
3127.201119	244870.908898	53.428506
3126.736108	244736.805091	53.433511
3126.012300	244606.638576	53.438516
3125.868369	244470.345142	53.443521
3125.006272	244332.382913	53.448525
3124.409444	244186.968448	53.453530
3123.484708	244050.340627	53.458535
3122.792776	243914.618327	53.463540
3122.102098	243780.143769	53.468545
3121.277980	243641.208590	53.473549
3120.296233	243508.715731	53.478554
3120.158861	243366.896479	53.483559
3119.489218	243225.696378	53.488564
3119.054123	243095.307453	53.493569
3118.102994	242964.185436	53.498573
3117.536751	242825.872442	53.503578
3117.148018	242685.545241	53.508583
3116.145212	242549.211512	53.513588
3115.575835	242415.661424	53.518593
3114.954869	242274.862140	53.523597
3114.014119	242139.996012	53.528602
3113.500821	241994.978304	53.533607
3112.843983	241867.095858	53.538612
3112.196443	241725.130033	53.543617
3111.205192	241612.172226	53.548621
3110.832588	241473.193503	53.553626
3110.144808	241328.153279	53.558631
3109.588619	241191.623084	53.563636
3108.603671	241054.702529	53.568641
3108.273253	240918.391569	53.573645
3107.555841	240782.473046	53.578650
3107.081168	240654.970511	53.583655
3106.300662	240516.057461	53.588660
3105.950399	240369.004241	53.593665
3104.903035	240239.402837	53.598669
3104.374462	240091.843432	53.603674
3103.524022	239963.458936	53.608679
3102.782079	239835.235666	53.613684
3102.326507	239687.614301	53.618689
3101.689375	239558.228862	53.623693
3101.220084	239410.049814	53.628698
3100.416950	239286.012996	53.633703
3099.735178	239147.035059	53.638708
3099.099478	239007.337007	53.643713
3098.059802	238873.712604	53.648717
3097.472201	238731.486333	53.653722
3097.100992	238595.490175	53.658727
3096.209114	238456.495423	53.663732
3095.929650	238327.818736	53.668737
3095.091252	238186.931523	53.673741
3094.400676	238055.060819	53.678746
3093.583984	237907.677215	53.683751
3092.799054	237785.650859	53.688756
3092.661659	237642.056103	53.693761
3091.608155	237516.278433	53.698765
3091.057936	237374.608225	53.703770
3090.442448	237234.501826	53.708775
3089.406451	237103.578185	53.713780
3088.611917	236959.095252	53.718785
3088.032567	236830.187713	53.723789
3087.407558	236707.042349	53.728794
3086.970859	236572.994353	53.733799
3086.093280	236439.449179	53.738804
3085.307370	236300.771492	53.743809
3084.912169	236186.120674	53.748813
3084.027974	236043.155546	53.753818
3083.601443	235908.164650	53.758823
3082.875948	235784.094134	53.763828
3082.489770	235649.504607	53.768833
3081.606133	235525.815920	53.773837
3081.054567	235384.377803	53.778842
3080.154278	235257.050819	53.783847
3079.438845	235129.694742	53.788852
3079.175278	234985.792594	53.793857
3078.025459	234861.077389	53.798861
3077.398141	234725.814283	53.803866
3077.362730	234589.108143	53.808871
3076.465616	234460.152029	53.813876
3075.664187	234321.224876	53.818881
3074.831612	234182.404699	53.823885
3074.335761	234055.804601	53.828890
3073.602494	233917.223714	53.833895
3072.729440	233779.479959	53.838900
3072.357727	233660.703312	53.843905
3071.719237	233528.601020	53.848909
3071.095850	233393.084498	53.853914
3070.609425	233259.761754	53.858919
3069.808894	233132.090713	53.863924
3068.821638	232988.484259	53.868929
3068.217123	232872.113460	53.873933
3067.999249	232730.600889	53.878938
3067.267576	232599.711367	53.883943
3066.299193	232468.350236	53.888948
3066.119357	232318.811543	53.893953
3065.108017	232191.022353	53.898957
3064.416706	232056.766146	53.903962
3063.962963	231925.451639	53.908967
3063.297216	231793.279684	53.913972
3062.713993	231653.481608	53.918977
3061.831403	231513.985744	53.923981
3061.140643	231377.667981	53.928986
3060.532765	231248.874130	53.933991
3059.504200	231122.769647	53.938996
3059.201700	230983.946647	53.944001
3058.361221	230853.509660	53.949005
3057.417427	230712.624283	53.954010
3057.164199	230582.654911	53.959015
3056.487449	230461.562618	53.964020
3056.075991	230318.964034	53.969025
3055.219770	230190.440144	53.974029
3054.916328	230059.970233	53.979034
3054.524998	229910.112464	53.984039
3053.259954	229785.804143	53.989044
3052.578133	229637.902445	53.994049
3051.507347	229504.932223	53.999053
3050.786684	229378.857842	54.004058
3050.231371	229233.279278	54.009063
3049.692299	229124.617780	54.014068
3049.266134	228981.743590	54.019073
3048.382482	228854.677293	54.024077
3047.559703	228727.041392	54.029082
3046.816770	228592.060130	54.034087
3045.583480	228480.021080	54.039092
3045.411505	228346.884908	54.044097
3045.063809	228221.364247	54.049101
3044.303469	228092.064412	54.054106
3043.778014	227961.556377	54.059111
3043.191266	227835.412119	54.064116
3042.766776	227707.612849	54.069121
3041.608574	227575.397800	54.074125
3040.645583	227438.059829	54.079130
3040.471986	227311.163510	54.084135
3039.679180	227190.297815	54.089140
3039.494080	227058.235097	54.094145
3038.586205	226935.338367	54.099149
3037.576301	226804.463221	54.104154
3037.112976	226672.139614	54.109159
3036.492713	226545.353338	54.114164
3035.869528	226410.445707	54.119169
3034.748468	226288.589376	54.124173
3034.579064	226159.122600	54.129178
3034.305651	226017.769599	54.134183
3033.024169	225893.571395	54.139188
3032.618105	225752.978204	54.144193
3031.808384	225627.063527	54.149197
3031.041950	225505.241345	54.154202
3030.688061	225370.343722	54.159207
3029.897979	225236.661083	54.164212
3029.536907	225093.821386	54.169217
3028.480090	224970.747486	54.174221
3027.725885	224834.195540	54.179226
3027.298151	224699.476217	54.184231
3026.251918	224567.299200	54.189236
3025.735615	224438.742990	54.194241
3025.094495	224316.660901	54.199245
3024.262410	224188.931612	54.204250
3023.642184	224055.287711	54.209255
3023.017928	223937.799086	54.214260
3022.431015	223808.924093	54.219265
3021.726921	223681.862787	54.224269
3021.233266	223554.170070	54.229274
3020.582859	223421.092142	54.234279
3019.804865	223291.789964	54.239284
3019.187543	223163.824670	54.244289
3018.415599	223039.804866	54.249293
3017.781492	222913.433878	54.254298
3017.048519	222778.078743	54.259303
3016.163246	222651.315123	54.264308
3015.903618	222520.531906	54.269313
3015.041229	222403.668860	54.274317
3014.274717	222282.755483	54.279322
3014.125089	222149.116752	54.284327
3013.032206	222025.658571	54.289332
3012.320878	221898.346749	54.294337
3011.786490	221775.322496	54.299341
3011.032403	221655.070093	54.304346
3010.353951	221528.797520	54.309351
3009.796062	221395.581166	54.314356
3009.431881	221264.460229	54.319361
3008.627127	221141.925339	54.324365
3008.105673	221010.626067	54.329370
3007.523479	220887.267135	54.334375
3006.397523	220765.687500	54.339380
3006.037779	220625.350819	54.344385
3005.407051	220505.258952	54.349389
3004.737174	220380.476312	54.354394
3003.945828	220246.458821	54.359399
3003.039541	220128.460620	54.364404
3002.612554	219997.148191	54.369409
3001.928764	219864.603710	54.374413
3001.158512	219745.718997	54.379418
3000.979510	219609.556325	54.384423
3000.100365	219483.726344	54.389428
2999.458220	219346.466378	54.394433
2998.827884	219229.597045	54.399437
2997.855558	219097.506969	54.404442
2997.320752	218970.197706	54.409447
2996.518042	218850.963183	54.414452
2996.150662	218708.441978	54.419457
2995.425516	218599.709873	54.424461
2994.730455	218464.853040	54.429466
2994.212408	218335.391033	54.434471
2993.382836	218213.590550	54.439476
2992.688051	218070.804216	54.444481
2991.801083	217950.642587	54.449485
2991.449942	217819.309395	54.454490
2990.700566	217693.996641	54.459495
2989.871989	217574.488316	54.464500
2989.413180	217446.291455	54.469505
2988.469876	217316.147624	54.474509
2987.886638	217191.382270	54.479514
2987.523800	217059.594112	54.484519
2986.684279	216937.250076	54.489524
2986.418283	216804.937917	54.494529
2985.318083	216674.743748	54.499533
2984.525602	216555.816982	54.504538
2984.354474	216425.972640	54.509543
2983.275075	216310.719403	54.514548
2982.703893	216178.393110	54.519553
2982.063031	216043.099594	54.524557
2981.165734	215929.294699	54.529562
2980.780010	215803.355012	54.534567
2979.979871	215679.135873	54.539572
2979.228702	215555.392895	54.544577
2978.658734	215428.159295	54.549581
2978.109419	215299.127942	54.554586
2977.406596	215168.657357	54.559591
2976.471162	215048.062959	54.564596
2976.160266	214919.198248	54.569601
2975.566494	214793.547942	54.574605
2974.598797	214671.037335	54.579610
2974.318665	214540.742900	54.584615
2973.432469	214420.243666	54.589620
2972.588240	214288.868008	54.594625
2972.028394	214170.188632	54.599629
2971.186733	214048.741127	54.604634
2970.354536	213923.626607	54.609639
2969.737918	213801.265683	54.614644
2969.052766	213679.857723	54.619649
2968.865413	213558.956683	54.624653
2967.949298	213434.912816	54.629658
2967.425208	213310.399826	54.634663
2966.724765	213191.477178	54.639668
2966.130702	213061.948130	54.644673
2965.111113	212935.363243	54.649677
2964.709865	212815.464771	54.654682
2964.090114	212697.268481	54.659687
2963.135148	212581.327415	54.664692
2962.836769	212445.477884	54.669697
2962.153893	212325.701269	54.674701
2961.327560	212204.343866	54.679706
2960.834565	212082.322986	54.684711
2959.966570	211965.134656	54.689716
2959.475618	211843.164819	54.694721
2958.684132	211724.870222	54.699725
2958.061815	211595.552238	54.704730
2957.700191	211468.980633	54.709735
2956.599151	211352.364888	54.714740
2956.272199	211220.315353	54.719745
2955.636680	211097.847994	54.724749
2954.800808	210972.192484	54.729754
2954.372316	210843.443553	54.734759
2953.529704	210731.777287	54.739764
2952.558558	210597.820067	54.744769
2952.109797	210472.193370	54.749773
2951.338178	210359.625598	54.754778
2950.759124	210230.685392	54.759783
2949.987733	210120.294424	54.764788
2949.072197	209988.060652	54.769793
2949.125871	209867.739360	54.774797
2947.866727	209746.149744	54.779802
2947.468733	209615.769406	54.784807
2946.724134	209499.317059	54.789812
2946.425705	209391.843453	54.794817
2945.525028	209264.738003	54.799821
2944.889794	209140.670803	54.804826
2944.359020	209007.627311	54.809831
2943.326375	208896.707165	54.814836
2942.648611	208768.727457	54.819841
2942.142314	208652.557175	54.824845
2941.377559	208529.058992	54.829850
2940.929750	208407.076325	54.834855
2940.306087	208293.114381	54.839860
2939.786529	208166.943602	54.844865
2939.124011	208043.493860	54.849869
2937.833433	207913.233008	54.854874
2937.871225	207789.380198	54.859879
2936.813587	207673.757252	54.864884
2936.102339	207547.643572	54.869889
2935.876353	207428.300434	54.874893
2934.702833	207298.862365	54.879898
2934.517741	207172.131651	54.884903
2933.801871	207062.450151	54.889908
2933.001203	206920.061561	54.894913
2932.241168	206812.080185	54.899917
2931.517746	206679.365054	54.904922
2931.063038	206555.350965	54.909927
2930.180345	206436.291958	54.914932
2929.515377	206312.871643	54.919937
2928.901346	206203.850130	54.924941
2928.213073	206080.001285	54.929946
2927.379530	205961.139088	54.934951
2926.777603	205841.947753	54.939956
2926.641937	205704.954719	54.944961
2925.592983	205597.644919	54.949965
2924.631681	205469.806276	54.954970
2924.606489	205343.550519	54.959975
2923.617886	205239.527990	54.964980
2922.988754	205099.496519	54.969985
2922.698394	204980.524881	54.974989
2922.000530	204853.702185	54.979994
2921.379670	204724.984077	54.984999
2920.503940	204608.651152	54.990004
2920.229931	204475.577189	54.995009
2919.376617	204351.007318	55.000013
2918.427653	204227.127353	55.005018
2917.805032	204090.444316	55.010023
2917.351789	203973.702190	55.015028
2916.529158	203837.165962	55.020033
2915.738425	203725.682777	55.025037
2914.762700	203604.137291	55.030042
2914.442281	203479.319524	55.035047
2913.639357	203364.377487	55.040052
2913.000922	203230.371500	55.045057
2912.250968	203117.966786	55.050061
2911.557862	202998.452201	55.055066
2911.529129	202878.832687	55.060071
2910.591480	202756.086766	55.065076
2909.699318	202628.396267	55.070081
2908.897525	202509.281712	55.075085
2907.877411	202383.584540	55.080090
2907.332233	202258.830525	55.085095
2906.695151	202154.808914	55.090100
2906.375770	202025.947423	55.095105
2905.592687	201919.276960	55.100109
2904.777123	201815.424227	55.105114
2904.317806	201687.896426	55.110119
2903.663284	201573.952642	55.115124
2902.934195	201444.444738	55.120129
2902.344123	201341.969742	55.125133
2901.797753	201221.570414	55.130138
2900.962520	201098.646526	55.135143
2899.962736	200977.988656	55.140148
2899.879751	200862.199743	55.145153
2899.306761	200740.138652	55.150157
2898.175700	200628.410163	55.155162
2897.585651	200505.245188	55.160167
2896.453778	200391.633956	55.165172
2896.216287	200275.438092	55.170177
2895.307695	200160.888494	55.175181
2894.808591	200052.318822	55.180186
2894.378706	199931.674854	55.185191
2893.365328	199827.933582	55.190196
2892.905543	199703.693616	55.195201
2892.486065	199594.883206	55.200205
2891.477346	199481.597978	55.205210
2891.230454	199348.939247	55.210215
2890.598914	199232.260845	55.215220
2890.040559	199113.802326	55.220225
2889.236758	198996.044634	55.225229
2888.404092	198880.022375	55.230234
2887.860032	198755.594359	55.235239
2886.838920	198645.468670	55.240244
2886.448276	198526.234136	55.245249
2885.813028	198405.180763	55.250253
2884.931030	198283.683190	55.255258
2884.156190	198172.883252	55.260263
2883.458131	198063.000303	55.265268
2882.985044	197933.269463	55.270273
2882.000315	197832.657858	55.275277
2881.554905	197713.039370	55.280282
2881.364689	197596.116562	55.285287
2880.133251	197484.995908	55.290292
2879.784809	197366.431733	55.295297
2879.215617	197243.780003	55.300301
2878.197787	197136.939919	55.305306
2878.016079	197024.063469	55.310311
2876.870171	196905.028559	55.315316
2876.455433	196784.109447	55.320321
2875.928094	196670.168737	55.325325
2874.991106	196559.372457	55.330330
2874.521324	196430.331965	55.335335
2873.702485	196321.095320	55.340340
2873.288438	196206.043401	55.345345
2872.799238	196086.371981	55.350349
2871.932495	195970.743327	55.355354
2871.334733	195845.045614	55.360359
2870.311602	195735.677150	55.365364
2870.024694	195612.322950	55.370369
2869.133586	195500.414693	55.375373
2868.395929	195388.596902	55.380378
2868.246676	195259.801268	55.385383
2867.130364	195143.705045	55.390388
2866.531974	195031.535165	55.395393
2865.869114	194911.105113	55.400397
2865.285180	194797.101202	55.405402
2864.628332	194679.482759	55.410407
2863.951136	194578.281716	55.415412
2863.216252	194444.758509	55.420417
2862.423979	194336.132680	55.425421
2861.746899	194219.103819	55.430426
2861.497759	194095.607380	55.435431
2860.359376	193987.342485	55.440436
2859.518226	193871.307427	55.445441
2859.053547	193761.587627	55.450445
2858.318829	193642.902432	55.455450
2857.951727	193535.165305	55.460455
2856.921677	193416.387455	55.465460
2856.187468	193290.056104	55.470465
2855.422350	193182.980776	55.475469
2855.150675	193074.847833	55.480474
2854.501668	192967.372880	55.485479
2853.413648	192863.759286	55.490484
2852.874097	192752.806673	55.495489
2852.406575	192627.376331	55.500493
2851.800696	192526.664394	55.505498
2850.995536	192409.469239	55.510503
2850.131360	192306.482996	55.515508
2849.936833	192187.410411	55.520513
2849.181279	192073.427214	55.525517
2848.592822	191973.922372	55.530522
2848.188842	191851.906522	55.535527
2847.060456	191734.318858	55.540532
2846.320342	191617.026248	55.545537
2845.644955	191503.209819	55.550541
2845.126438	191401.812048	55.555546
2844.906593	191286.015526	55.560551
2843.726714	191173.157654	55.565556
2843.073891	191063.410074	55.570561
2842.473656	190948.577933	55.575565
2841.784226	190837.895161	55.580570
2841.278076	190729.066620	55.585575
2840.422448	190618.245274	55.590580
2840.063439	190505.856965	55.595585
2839.088776	190391.759761	55.600589
2838.632648	190271.715490	55.605594
2837.971744	190154.197617	55.610599
2837.025431	190056.712717	55.615604
2836.510793	189934.452074	55.620609
2836.062419	189819.598597	55.625613
2835.373103	189716.946443	55.630618
2834.951022	189599.239453	55.635623
2833.779960	189487.580103	55.640628
2833.604442	189368.587825	55.645633
2832.674367	189257.832330	55.650637
2832.028358	189151.014269	55.655642
2831.497609	189029.381919	55.660647
2830.583444	188920.240459	55.665652
2830.055275	188802.857595	55.670657
2829.583430	188691.013079	55.675661
2828.430321	188581.057844	55.680666
2827.880013	188465.269630	55.685671
2827.322195	188354.597267	55.690676
2826.422141	188242.923410	55.695681
2825.949810	188125.571571	55.700685
2825.260190	188021.587336	55.705690
2824.433145	187905.857057	55.710695
2823.647955	187798.160851	55.715700
2823.297128	187681.605113	55.720705
2822.724387	187577.908695	55.725709
2821.695378	187468.025498	55.730714
2821.378161	187353.195467	55.735719
2820.483450	187248.533012	55.740724
2820.200565	187141.852887	55.745729
2819.383229	187036.529839	55.750733
2818.410912	186927.898429	55.755738
2817.841108	186807.881043	55.760743
2816.846280	186703.922666	55.765748
2816.239301	186582.588684	55.770753
2815.847951	186482.975165	55.775757
2814.974622	186386.707686	55.780762
2814.949853	186278.118594	55.785767
2814.185061	186161.543213	55.790772
2813.394775	186048.508798	55.795777
2812.735170	185936.128217	55.800781
2811.755288	185832.144020	55.805786
2811.429171	185720.817943	55.810791
2810.703288	185618.638645	55.815796
2809.983515	185514.728481	55.820801
2809.380146	185399.885069	55.825805
2808.636489	185292.697050	55.830810
2807.797640	185176.848336	55.835815
2807.301316	185069.647123	55.840820
2806.563030	184954.966146	55.845825
2805.980612	184859.788053	55.850829
2805.105237	184750.434114	55.855834
2804.798053	184641.155839	55.860839
2804.270591	184537.917150	55.865844
2803.449376	184423.594141	55.870849
2803.020735	184310.366885	55.875853
2801.940981	184191.772929	55.880858
2801.589400	184075.837179	55.885863
2800.577993	183976.518211	55.890868
2800.138525	183865.927069	55.895873
2799.353139	183760.644772	55.900877
2798.088301	183653.097989	55.905882
2798.275494	183542.929973	55.910887
2797.451731	183432.527981	55.915892
2796.709709	183321.718973	55.920897
2796.418958	183220.786508	55.925901
2795.485521	183111.789265	55.930906
2794.862965	183002.946592	55.935911
2794.388140	182890.824271	55.940916
2794.049053	182766.646906	55.945921
2793.015934	182656.458109	55.950925
2792.387507	182542.745472	55.955930
2791.756695	182426.387612	55.960935
2790.893214	182323.601652	55.965940
2790.329956	182212.665371	55.970945
2789.538426	182097.364210	55.975949
2788.770822	181985.290579	55.980954
2788.134808	181877.470483	55.985959
2787.071949	181769.183995	55.990964
2786.813421	181656.432729	55.995969
2785.929699	181553.041218	56.000973
2785.292196	181455.017118	56.005978
2784.601934	181347.970154	56.010983
2783.983754	181246.992348	56.015988
2783.498428	181137.064102	56.020993
2782.702575	181023.369242	56.025997
2782.054841	180907.666873	56.031002
2781.644454	180801.988885	56.036007
2781.037457	180706.645615	56.041012
2780.611869	180584.536139	56.046017
2779.667002	180480.508165	56.051021
2779.006477	180368.548980	56.056026
2778.660575	180247.254650	56.061031
2778.046280	180138.557791	56.066036
2777.111085	180021.783984	56.071041
2776.350627	179919.051049	56.076045
2775.496355	179811.245266	56.081050
2775.072117	179700.903999	56.086055
2774.144070	179592.754300	56.091060
2773.734671	179471.841111	56.096065
2772.989039	179360.457731	56.101069
2772.236453	179257.737871	56.106074
2771.696761	179150.698011	56.111079
2770.918466	179046.850685	56.116084
2769.951721	178932.857765	56.121089
2769.221794	178827.782236	56.126093
2768.688450	178714.904188	56.131098
2768.397076	178611.896627	56.136103
2767.379627	178513.367099	56.141108
2766.838109	178399.104770	56.146113
2766.375046	178300.030041	56.151117
2765.270961	178207.505806	56.156122
2764.878948	178096.006176	56.161127
2764.075298	177993.055833	56.166132
2763.787365	177888.612224	56.171137
2762.900563	177783.246183	56.176141
2762.740945	177673.567889	56.181146
2762.018874	177551.018100	56.186151
2761.225849	177445.777974	56.191156
2760.553785	177328.906390	56.196161
2759.915727	177218.770870	56.201165
2758.937066	177104.797556	56.206170
2758.469699	176991.621190	56.211175
2757.436306	176896.074277	56.216180
2756.481539	176786.015512	56.221185
2756.148107	176682.892202	56.226189
2755.601815	176587.841210	56.231194
2755.247283	176479.735941	56.236199
2754.057057	176378.822271	56.241204
2753.497394	176271.475015	56.246209
2753.127121	176160.295131	56.251213
2752.321435	176054.907942	56.256218
2751.733342	175949.308501	56.261223
2751.182033	175846.857737	56.266228
2750.505145	175739.886567	56.271233
2749.818957	175631.352761	56.276237
2749.173451	175523.194359	56.281242
2748.826910	175399.879272	56.286247
2747.822841	175305.119986	56.291252
2747.379203	175175.474427	56.296257
2746.700778	175072.117302	56.301261
2745.736061	174970.370149	56.306266
2745.468433	174856.532143	56.311271
2744.798225	174750.134852	56.316276
2744.022331	174634.139550	56.321281
2743.320792	174518.857746	56.326285
2742.444920	174407.800898	56.331290
2741.955635	174299.125017	56.336295
2741.106734	174189.806892	56.341300
2740.502083	174089.963531	56.346305
2739.883752	173972.647935	56.351309
2738.988657	173878.854041	56.356314
2738.811382	173754.029166	56.361319
2737.755901	173656.496666	56.366324
2737.173328	173536.378731	56.371329
2736.491667	173433.000903	56.376333
2735.848619	173320.600253	56.381338
2735.465450	173217.150273	56.386343
2734.490766	173132.514873	56.391348
2733.989758	173010.338039	56.396353
2733.065667	172909.187432	56.401357
2732.276416	172801.644153	56.406362
2731.717132	172687.616880	56.411367
2731.126027	172588.614509	56.416372
2730.788066	172483.073591	56.421377
2730.002776	172367.048225	56.426381
2728.974951	172256.530156	56.431386
2728.387240	172156.790714	56.436391
2727.864385	172056.481685	56.441396
2727.286179	171944.227289	56.446401
2726.818633	171832.769600	56.451405
2725.692329	171735.609149	56.456410
2724.908638	171629.734168	56.461415
2724.579432	171525.987579	56.466420
2723.665354	171417.285151	56.471425
2723.024019	171318.675457	56.476429
2722.593398	171220.808386	56.481434
2722.115564	171102.423536	56.486439
2721.312320	171000.533832	56.491444
2720.802377	170887.597653	56.496449
2720.300100	170783.715131	56.501453
2719.272420	170675.605039	56.506458
2718.696833	170568.212091	56.511463
2717.909279	170461.997542	56.516468
2717.480341	170339.690454	56.521473
2716.656099	170238.352908	56.526477
2716.145530	170134.537027	56.531482
2715.502286	170018.216385	56.536487
2714.603255	169917.501937	56.541492
2714.016156	169809.426219	56.546497
2713.581970	169708.244468	56.551501
2712.889402	169599.677378	56.556506
2712.109674	169484.791521	56.561511
2711.166525	169386.463464	56.566516
2710.660207	169273.111791	56.571521
2709.794013	169167.154892	56.576525
2709.016088	169066.474364	56.581530
2708.444240	168961.005504	56.586535
2707.942047	168862.710681	56.591540
2707.617779	168745.923735	56.596545
2706.950820	168638.054723	56.601549
2706.038595	168536.761052	56.606554
2705.173965	168424.727575	56.611559
2704.418196	168325.584168	56.616564
2704.210316	168210.916759	56.621569
2703.401961	168105.678481	56.626573
2702.506221	168010.754407	56.631578
2702.297388	167900.042809	56.636583
2701.355836	167798.781192	56.641588
2701.148280	167693.652350	56.646593
2700.630192	167574.407376	56.651597
2699.536273	167468.605742	56.656602
2699.079406	167359.295629	56.661607
2698.036025	167260.213299	56.666612
2697.617585	167144.031149	56.671617
2696.911643	167038.334578	56.676621
2696.431446	166930.580738	56.681626
2695.877349	166814.586404	56.686631
2695.105765	166705.684091	56.691636
2694.338115	166596.463582	56.696641
2693.588544	166487.405831	56.701645
2692.703707	166378.573277	56.706650
2692.373399	166274.764849	56.711655
2691.537490	166164.437452	56.716660
2690.883242	166054.348631	56.721665
2690.194362	165939.764358	56.726669
2689.274189	165845.065815	56.731674
2688.904629	165732.504211	56.736679
2688.574121	165631.520424	56.741684
2687.666638	165521.994629	56.746689
2687.152072	165415.662021	56.751693
2686.387178	165306.724610	56.756698
2686.203978	165188.527731	56.761703
2685.247524	165084.364083	56.766708
2684.689654	164962.272875	56.771713
2683.847365	164847.919736	56.776717
2683.223552	164741.237646	56.781722
2682.500322	164636.822168	56.786727
2681.741015	164525.724641	56.791732
2681.107180	164417.341279	56.796737
2680.455159	164298.954518	56.801741
2679.239752	164199.704203	56.806746
2679.260146	164089.819544	56.811751
2678.018504	163987.140969	56.816756
2677.638018	163886.182616	56.821761
2676.857116	163774.671211	56.826765
2676.342160	163669.627918	56.831770
2675.660008	163561.877773	56.836775
2674.992927	163455.714883	56.841780
2674.427733	163339.161104	56.846785
2674.033284	163229.955057	56.851789
2673.249060	163127.270029	56.856794
2672.722911	163011.664704	56.861799
2671.815652	162905.109188	56.866804
2670.977991	162798.275960	56.871809
2671.029605	162678.651443	56.876813
2669.835558	162570.336919	56.881818
2669.196262	162460.307419	56.886823
2668.585846	162354.100651	56.891828
2667.551018	162247.452866	56.896833
2667.041817	162134.377790	56.901837
2666.400596	162029.791554	56.906842
2666.003807	161921.670543	56.911847
2665.099713	161817.279141	56.916852
2664.411356	161709.014253	56.921857
2664.012140	161591.435443	56.926861
2663.068346	161484.622947	56.931866
2662.702080	161372.837167	56.936871
2662.009036	161271.694099	56.941876
2661.440686	161160.017284	56.946881
2660.844147	161052.248398	56.951885
2660.043382	160932.815607	56.956890
2659.911166	160821.325038	56.961895
2658.931686	160709.168088	56.966900
2658.243656	160597.956979	56.971905
2657.641122	160490.534019	56.976909
2657.001593	160375.323882	56.981914
2656.484428	160252.479389	56.986919
2655.802641	160146.226955	56.991924
2655.068512	160014.759841	56.996929
2654.305753	159899.138531	57.001933
2653.635198	159792.160729	57.006938
2653.047611	159674.643557	57.011943
2651.924601	159565.983700	57.016948
2651.681435	159444.865755	57.021953
2651.052493	159324.305156	57.026957
2650.170530	159218.468639	57.031962
2649.424861	159098.906216	57.036967
2648.829048	158992.008012	57.041972
2647.952586	158879.738886	57.046977
2647.451689	158773.614517	57.051981
2646.612810	158673.887734	57.056986
2646.157642	158549.806247	57.061991
2645.387741	158443.839918	57.066996
2644.826661	158333.162542	57.072001
2644.133742	158216.340749	57.077005
2643.444064	158102.747850	57.082010
2643.236520	157990.273927	57.087015
2642.119199	157888.775615	57.092020
2641.871749	157769.176980	57.097025
2641.183159	157653.958182	57.102029
2640.114961	157538.138862	57.107034
2639.661163	157415.777407	57.112039
2639.174369	157312.121493	57.117044
2638.088206	157191.005136	57.122049
2637.450843	157103.340381	57.127053
2636.519263	156982.085861	57.132058
2636.150090	156867.327586	57.137063
2635.444018	156764.877589	57.142068
2634.709812	156643.732832	57.147073
2634.225896	156535.121090	57.152077
2633.389305	156441.451361	57.157082
2632.922120	156321.892583	57.162087
2631.853003	156213.832211	57.167092
2631.384931	156105.638821	57.172097
2631.039963	155986.773724	57.177101
2630.379241	155885.120035	57.182106
2629.738429	155765.819533	57.187111
2628.844549	155659.500101	57.192116
2628.219671	155551.740096	57.197121
2627.616780	155430.070391	57.202125
2626.504546	155335.468590	57.207130
2626.051241	155217.449611	57.212135
2625.250629	155120.663496	57.217140
2624.924894	155017.116169	57.222145
2624.312235	154904.640325	57.227149
2623.435158	154795.448163	57.232154
2623.026155	154686.665228	57.237159
2622.342633	154580.201468	57.242164
2621.775556	154462.508233	57.247169
2620.749223	154345.460180	57.252173
2620.170663	154246.429645	57.257178
2619.995473	154130.061010	57.262183
2619.185015	154015.089964	57.267188
2618.690740	153897.870202	57.272193
2618.062785	153790.472241	57.277197
2617.436852	153673.134307	57.282202
2616.670318	153550.455041	57.287207
2615.948796	153448.437029	57.292212
2615.204616	153325.691496	57.297217
2614.692876	153211.807161	57.302221
2613.920646	153103.417412	57.307226
2613.147422	152988.405882	57.312231
2612.770832	152869.988998	57.317236
2611.922142	152759.832991	57.322241
2611.375067	152640.694011	57.327245
2610.379025	152529.189376	57.332250
2609.733716	152402.478617	57.337255
2609.306561	152293.744507	57.342260
2608.609516	152184.112947	57.347265
2608.138907	152072.399503	57.352269
2607.077970	151984.179713	57.357274
2607.101162	151787.509405	57.362279
2606.565521	151668.600915	57.367284
2605.419375	151548.709220	57.372289
2604.865891	151427.440338	57.377293
2603.943199	151315.623159	57.382298
2603.606973	151196.786467	57.387303
2602.736899	151079.712512	57.392308
2601.804645	150978.027874	57.397313
2601.676685	150846.462213	57.402317
2600.810435	150749.267139	57.407322
2600.180150	150605.504312	57.412327
2599.512556	150500.131518	57.417332
2599.064934	150378.671828	57.422337
2598.477036	150258.289722	57.427341
2597.708819	150143.350936	57.432346
2597.125439	150009.878119	57.437351
2596.022326	149904.372917	57.442356
2595.312082	149778.572299	57.447361
2594.991685	149666.449307	57.452365
2593.971644	149558.352057	57.457370
2593.498283	149435.260476	57.462375
2592.788153	149331.207296	57.467380
2592.038856	149205.173628	57.472385
2591.427870	149105.439329	57.477389
2590.786746	148979.427534	57.482394
2590.298113	148860.102491	57.487399
2589.202463	148750.888828	57.492404
2588.474553	148625.642012	57.497409
2588.067309	148514.388306	57.502413
2587.395211	148417.194922	57.507418
2586.777441	148285.234373	57.512423
2586.469770	148185.772602	57.517428
2585.448136	148063.306937	57.522433
2584.680965	147945.033441	57.527437
2584.221236	147834.502114	57.532442
2583.776494	147713.776441	57.537447
2582.763330	147609.789593	57.542452
2582.503323	147488.171320	57.547457
2581.538505	147370.376083	57.552461
2580.690000	147260.899622	57.557466
2580.212177	147136.521345	57.562471
2579.689959	147021.859801	57.567476
2579.020361	146895.301600	57.572481
2578.442366	146786.343088	57.577485
2577.483263	146667.443946	57.582490
2577.300780	146530.973838	57.587495
2576.274090	146431.923794	57.592500
2575.583956	146310.238422	57.597505
2574.663913	146194.117956	57.602509
2574.182909	146085.858153	57.607514
2573.535287	145977.968240	57.612519
2572.941249	145866.461157	57.617524
2572.386589	145738.453407	57.622529
2571.619094	145637.687364	57.627533
2571.033396	145519.813572	57.632538
2570.583785	145386.529595	57.637543
2569.583369	145270.272804	57.642548
2568.761889	145158.130784	57.647553
2568.506125	145030.764787	57.652557
2567.701892	144933.158325	57.657562
2567.256676	144808.873068	57.662567
2566.559147	144685.962571	57.667572
2565.839887	144564.085304	57.672577
2565.038330	144439.934235	57.677581
2564.125072	144341.177838	57.682586
2564.023949	144215.328267	57.687591
2563.139453	144104.902813	57.692596
2562.286758	143990.711396	57.697601
2561.749748	143863.559955	57.702605
2560.974612	143755.710673	57.707610
2560.609140	143628.228051	57.712615
2559.732987	143524.588900	57.717620
2559.178550	143403.846431	57.722625
2558.684677	143285.788695	57.727629
2557.659201	143171.373563	57.732634
2557.338325	143032.628104	57.737639
2556.870342	142929.142300	57.742644
2556.003156	142798.197454	57.747649
2555.523412	142673.138468	57.752653
2554.731802	142560.289596	57.757658
2553.920349	142436.237137	57.762663
2553.328188	142324.539238	57.767668
2552.836785	142194.020282	57.772673
2552.192436	142070.717923	57.777677
2551.190150	141954.397726	57.782682
2550.634557	141826.088714	57.787687
2549.852720	141708.489312	57.792692
2549.135716	141602.734945	57.797697
2548.896253	141478.265396	57.802701
2547.908851	141363.825613	57.807706
2547.501411	141227.452718	57.812711
2546.791861	141119.183071	57.817716
2546.316605	140990.509102	57.822721
2545.648636	140873.657258	57.827725
2544.935163	140748.833829	57.832730
2544.137527	140627.086343	57.837735
2543.740162	140494.857242	57.842740
2542.641892	140379.612896	57.847745
2542.305155	140256.840948	57.852749
2541.473261	140133.245875	57.857754
2541.012343	140020.404903	57.862759
2540.048177	139892.118046	57.867764
2539.273538	139776.850146	57.872769
2539.177451	139654.055238	57.877773
2538.175955	139534.199480	57.882778
2537.663663	139409.794433	57.887783
2537.159907	139283.088914	57.892788
2536.477276	139154.138061	57.897793
2535.970777	139040.977681	57.902797
2534.861274	138915.970560	57.907802
2534.440145	138787.907323	57.912807
2533.902579	138668.680307	57.917812
2532.933806	138531.201682	57.922817
2532.620858	138408.077840	57.927821
2531.541458	138286.905457	57.932826
2531.058448	138156.949040	57.937831
2530.498964	138032.811339	57.942836
2530.018972	137919.549406	57.947841
2528.845161	137790.136035	57.952845
2528.235857	137672.715747	57.957850
2527.872572	137534.586813	57.962855
2527.082720	137422.481184	57.967860
2526.391713	137291.303813	57.972865
2525.825624	137162.825948	57.977869
2524.857851	137046.443203	57.982874
2524.156562	136912.105806	57.987879
2523.764522	136793.180923	57.992884
2522.923842	136671.215128	57.997889
2522.640456	136533.357737	58.002893
2521.770354	136431.596979	58.007898
2521.253425	136297.449159	58.012903
2520.380904	136177.484987	58.017908
2519.860416	136045.612880	58.022913
2519.308826	135913.974967	58.027917
2518.415735	135788.934165	58.032922
2517.960072	135675.778693	58.037927
2517.392333	135554.866833	58.042932
2516.398715	135423.974485	58.047937
2516.461472	135293.143978	58.052941
2515.147892	135170.624253	58.057946
2514.760695	135030.656272	58.062951
2513.941205	134914.195049	58.067956
2513.294556	134780.951331	58.072961
2512.884356	134638.333922	58.077965
2512.085412	134522.023467	58.082970
2511.430483	134399.466155	58.087975
2510.759683	134263.446688	58.092980
2510.205236	134140.582387	58.097985
2509.505392	134000.440310	58.102989
2508.509972	133883.007620	58.107994
2507.962253	133759.343608	58.112999
2506.983757	133628.164872	58.118004
2506.371596	133511.498646	58.123009
2506.232619	133380.607185	58.128013
2505.328739	133261.434988	58.133018
2504.913269	133133.726013	58.138023
2504.247941	133019.483702	58.143028
2503.673875	132873.877866	58.148033
2502.660195	132746.049497	58.153037
2501.895871	132624.901691	58.158042
2501.439011	132491.155876	58.163047
2500.820468	132357.321997	58.168052
2499.828596	132235.246555	58.173057
2499.298865	132113.149205	58.178061
2498.478437	131987.643512	58.183066
2498.000259	131859.962910	58.188071
2497.503389	131735.601039	58.193076
2496.639487	131607.842990	58.198081
2496.122311	131483.625168	58.203085
2495.283947	131357.197895	58.208090
2495.136359	131217.502800	58.213095
2494.134699	131107.830604	58.218100
2493.448169	130969.543124	58.223105
2493.133671	130847.074209	58.228109
2492.141172	130720.420203	58.233114
2491.989678	130574.149591	58.238119
2490.945790	130454.109642	58.243124
2490.268287	130309.676561	58.248129
2489.856260	130181.840690	58.253133
2488.963526	130059.720891	58.258138
2488.225300	129925.422220	58.263143
2487.507806	129787.221703	58.268148
2486.755430	129669.374309	58.273153
2486.273175	129546.074024	58.278157
2485.452541	129416.642611	58.283162
2485.005545	129286.809663	58.288167
2484.283641	129165.949495	58.293172
2483.489384	129036.579180	58.298177
2482.960986	128895.076368	58.303181
2482.119891	128775.430653	58.308186
2481.810733	128641.171800	58.313191
2481.193611	128520.348649	58.318196
2480.278921	128387.215739	58.323201
2479.892303	128255.942922	58.328205
2479.201233	128125.290495	58.333210
2478.393450	127989.589818	58.338215
2477.916438	127863.400570	58.343220
2477.297622	127729.550845	58.348225
2476.595254	127597.289814	58.353229
2475.508344	127467.630356	58.358234
2475.277347	127327.485460	58.363239
2474.406712	127203.927010	58.368244
2473.982658	127080.653930	58.373249
2473.444245	126935.644963	58.378253
2472.633696	126811.697774	58.383258
2472.079663	126675.988792	58.388263
2471.239849	126543.894342	58.393268
2470.563939	126401.602304	58.398273
2470.248523	126271.254780	58.403277
2469.347763	126144.645362	58.408282
2468.810756	125998.790309	58.413287
2467.993436	125867.025767	58.418292
2467.225537	125736.638238	58.423297
2466.652289	125597.585123	58.428301
2465.943161	125468.789651	58.433306
2465.595858	125327.403595	58.438311
2464.641617	125194.381442	58.443316
2463.749615	125060.816731	58.448321
2463.340915	124921.220368	58.453325
2462.337782	124796.055757	58.458330
2461.808120	124667.248370	58.463335
2460.961812	124536.980661	58.468340
2460.136547	124397.960985	58.473345
2460.089680	124277.625031	58.478349
2459.086678	124156.679265	58.483354
2458.717627	124013.906739	58.488359
2457.761927	123891.303895	58.493364
2457.466972	123745.638552	58.498369
2456.744642	123613.184299	58.503373
2455.637580	123486.835962	58.508378
2455.141878	123354.118509	58.513383
2454.590196	123239.352781	58.518388
2453.975371	123101.525499	58.523393
2453.398116	122971.146595	58.528397
2452.622568	122846.247098	58.533402
2452.095410	122699.341809	58.538407
2451.133329	122580.237883	58.543412
2450.825299	122440.041740	58.548417
2450.436152	122314.639087	58.553421
2449.271224	122184.192136	58.558426
2448.843316	122043.788541	58.563431
2448.322781	121902.498865	58.568436
2447.669794	121770.677686	58.573441
2447.114693	121638.651194	58.578445
2446.116107	121501.807271	58.583450
2445.472428	121371.522966	58.588455
2444.679064	121231.829175	58.593460
2444.238979	121096.155838	58.598465
2444.140844	120955.413745	58.603469
2442.730853	120823.311012	58.608474
2442.107011	120691.744563	58.613479
2441.752939	120550.740490	58.618484
2441.026042	120426.606556	58.623489
2440.357784	120286.117138	58.628493
2439.806276	120145.578229	58.633498
2439.636126	120005.233555	58.638503
2438.524875	119866.727422	58.643508
2437.419951	119735.521371	58.648513
2437.184723	119585.686128	58.653517
2436.496268	119465.835641	58.658522
2435.438012	119310.812769	58.663527
2435.495170	119174.740505	58.668532
2434.434293	119035.576980	58.673537
2434.252978	118899.042476	58.678541
2433.062137	118749.363542	58.683546
2432.644477	118597.906127	58.688551
2431.755200	118469.332057	58.693556
2431.129289	118331.620506	58.698561
2430.570840	118189.798350	58.703565
2429.537096	118062.074421	58.708570
2429.209021	117918.611269	58.713575
2428.706927	117788.887423	58.718580
2427.882661	117639.334568	58.723585
2427.343594	117498.160613	58.728589
2426.406944	117358.326314	58.733594
2425.857789	117217.453838	58.738599
2424.979695	117086.384002	58.743604
2424.209921	116947.401449	58.748609
2423.700121	116807.521542	58.753613
2423.131448	116670.000262	58.758618
2422.312232	116529.726610	58.763623
2421.460735	116399.633577	58.768628
2420.987323	116273.365807	58.773633
2420.578086	116131.087096	58.778637
2419.843493	116003.821120	58.783642
2419.125098	115859.517401	58.788647
2418.429700	115713.490785	58.793652
2417.671953	115576.970154	58.798657
2417.343248	115438.268674	58.803661
2416.553262	115311.871808	58.808666
2415.935592	115168.051131	58.813671
2415.257042	115039.010308	58.818676
2414.775729	114889.768335	58.823681
2413.867358	114749.721772	58.828685
2412.848302	114626.830055	58.833690
2412.708949	114473.017376	58.838695
2411.812521	114344.262177	58.843700
2410.929664	114226.193430	58.848705
2410.490595	114067.949929	58.853709
2409.861707	113945.551860	58.858714
2409.312121	113807.332296	58.863719
2408.248800	113662.232694	58.868724
2407.713289	113532.059932	58.873729
2407.329603	113399.249000	58.878733
2406.645073	113271.849273	58.883738
2406.008266	113127.123076	58.888743
2405.424065	112975.160779	58.893748
2404.787125	112840.641349	58.898753
2404.282867	112703.747108	58.903757
2403.525198	112565.377017	58.908762
2402.784201	112426.116572	58.913767
2401.954023	112285.804873	58.918772
2401.417557	112147.757435	58.923777
2400.968282	112001.916507	58.928781
2399.980764	111853.896187	58.933786
2399.627792	111724.567024	58.938791
2398.702777	111599.923792	58.943796
2397.917493	111445.356424	58.948801
2397.647168	111308.877028	58.953805
2397.156483	111165.211594	58.958810
2396.477399	111018.410239	58.963815
2395.485466	110874.013686	58.968820
2394.909500	110733.397635	58.973825
2394.333150	110594.616394	58.978829
2393.622896	110453.217315	58.983834
2392.928737	110303.053007	58.988839
2392.315370	110166.031489	58.993844
2391.392216	110023.666016	58.998849
2390.818591	109878.910763	59.003853
2390.128783	109749.664424	59.008858
2389.543563	109609.995440	59.013863
2388.494836	109469.290266	59.018868
2388.169889	109324.416384	59.023873
2387.410167	109183.698771	59.028877
2386.825439	109047.053377	59.033882
2386.222629	108909.700933	59.038887
2385.840863	108772.853579	59.043892
2384.935560	108623.507219	59.048897
2384.188218	108479.054332	59.053901
2383.741191	108340.538262	59.058906
2383.286274	108199.613055	59.063911
2382.249043	108065.310170	59.068916
2381.778097	107916.203882	59.073921
2381.196369	107766.938414	59.078925
2379.936034	107642.171865	59.083930
2379.764211	107487.684605	59.088935
2379.231321	107351.878107	59.093940
2378.314452	107213.265331	59.098945
2377.945190	107066.261049	59.103949
2376.927280	106930.235615	59.108954
2376.431067	106776.978148	59.113959
2375.925004	106636.774467	59.118964
2375.108572	106492.794922	59.123969
2374.615765	106345.630643	59.128973
2373.479807	106213.637858	59.133978
2373.218364	106063.805589	59.138983
2372.420217	105919.629912	59.143988
2371.671152	105781.036893	59.148993
2370.931137	105637.481819	59.153997
2370.431437	105496.420964	59.159002
2369.391934	105348.245567	59.164007
2369.044191	105229.888053	59.169012
2368.541026	105080.975816	59.174017
2368.231034	104932.903061	59.179021
2367.015162	104795.309725	59.184026
2366.278386	104655.636444	59.189031
2365.894174	104508.244256	59.194036
2365.515697	104367.151861	59.199041
2364.687692	104216.463085	59.204045
2363.757149	104085.629576	59.209050
2363.320502	103930.268406	59.214055
2362.712135	103794.037381	59.219060
2361.887348	103642.875956	59.224065
2361.456330	103498.358638	59.229069
2360.237840	103367.333703	59.234074
2359.817790	103224.941541	59.239079
2359.285513	103075.240892	59.244084
2358.622262	102928.530865	59.249089
2357.926307	102785.791795	59.254093
2357.050582	102654.412000	59.259098
2356.422780	102502.719191	59.264103
2356.155162	102367.311507	59.269108
2355.183362	102221.035454	59.274113
2354.418486	102062.858685	59.279117
2353.948802	101927.016167	59.284122
2353.099942	101784.326490	59.289127
2352.475184	101651.783408	59.294132
2351.830261	101512.957946	59.299137
2351.165002	101372.480914	59.304141
2350.730058	101227.109214	59.309146
2350.318462	101076.336570	59.314151
2349.706954	100938.105518	59.319156
2348.623291	100791.558062	59.324161
2348.257002	100640.838157	59.329165
2347.291037	100502.056962	59.334170
2346.842975	100356.604000	59.339175
2345.871140	100204.879246	59.344180
2345.319082	100073.392960	59.349185
2344.967943	99911.600486	59.354189
2343.951679	99787.255517	59.359194
2343.625637	99624.909242	59.364199
2343.109726	99489.246929	59.369204
2342.014747	99334.337949	59.374209
2341.738585	99188.211800	59.379213
2340.688350	99052.941237	59.384218
2340.167014	98900.544762	59.389223
2339.447229	98759.121860	59.394228
2338.941437	98608.158309	59.399233
2338.523259	98463.061437	59.404237
2337.179376	98320.091134	59.409242
2336.823147	98174.795995	59.414247
2336.419951	98032.610693	59.419252
2335.764490	97885.544554	59.424257
2335.078860	97731.748541	59.429261
2334.488147	97590.857862	59.434266
2333.402046	97431.362191	59.439271
2333.131000	97293.130834	59.444276
2332.088527	97146.219636	59.449281
2331.772725	96991.520140	59.454285
2330.662319	96860.147214	59.459290
2330.245277	96707.761562	59.464295
2329.688714	96562.616315	59.469300
2328.890555	96414.554929	59.474305
2328.454773	96265.599916	59.479309
2327.387502	96120.113579	59.484314
2327.054016	95983.491949	59.489319
2326.140873	95834.869148	59.494324
2325.672390	95693.025977	59.499329
2325.055602	95543.647829	59.504333
2324.071395	95392.844968	59.509338
2323.405963	95254.130558	59.514343
2322.988539	95118.599238	59.519348
2322.173399	94960.752275	59.524353
2321.539196	94817.190634	59.529357
2320.981367	94672.159256	59.534362
2320.493980	94520.287876	59.539367
2319.933379	94367.604752	59.544372
2319.059834	94233.983789	59.549377
2318.262330	94075.055909	59.554381
2317.738277	93946.295803	59.559386
2316.931097	93792.679153	59.564391
2316.557719	93648.506620	59.569396
2315.806708	93502.188168	59.574401
2314.990427	93352.393400	59.579405
2314.186486	93210.752345	59.584410
2313.564052	93058.791871	59.589415
2312.976713	92921.081486	59.594420
2312.336703	92772.664052	59.599425
2311.785037	92611.501010	59.604429
2310.992521	92490.039613	59.609434
2310.653969	92324.970580	59.614439
2309.803274	92188.048401	59.619444
2309.241767	92039.319089	59.624449
2308.806024	91883.564339	59.629453
2308.014556	91753.680015	59.634458
2307.543155	91587.667444	59.639463
2306.736762	91448.574344	59.644468
2305.701246	91290.858203	59.649473
2305.240429	91139.411597	59.654477
2304.430279	90996.048461	59.659482
2303.896590	90847.658851	59.664487
2303.347994	90703.133904	59.669492
2302.647424	90553.555398	59.674497
2301.787767	90399.717103	59.679501
2300.973415	90258.388366	59.684506
2300.654049	90101.131529	59.689511
2300.142784	89966.857655	59.694516
2299.153896	89814.109133	59.699521
2298.754837	89669.624382	59.704525
2298.024436	89524.717629	59.709530
2297.406515	89369.180853	59.714535
2296.541918	89214.774778	59.719540
2295.799878	89076.288895	59.724545
2295.447347	88931.858734	59.729549
2294.539598	88783.561529	59.734554
2293.894767	88637.620085	59.739559
2292.889831	88486.798075	59.744564
2292.451231	88342.968750	59.749569
2292.045044	88194.970092	59.754573
2291.358597	88047.194400	59.759578
2290.447179	87907.627096	59.764583
2290.211227	87762.596687	59.769588
2289.298270	87612.267034	59.774593
2288.873568	87459.261839	59.779597
2288.121973	87321.600183	59.784602
2287.642369	87154.424647	59.789607
2286.838259	87002.725382	59.794612
2285.872701	86859.116327	59.799617
2285.464803	86700.643100	59.804621
2284.530039	86560.321218	59.809626
2284.251372	86404.517499	59.814631
2283.385772	86258.025009	59.819636
2282.869589	86114.476480	59.824641
2281.983907	85964.724586	59.829645
2281.285122	85815.768170	59.834650
2280.618756	85667.625374	59.839655
2279.815691	85524.405227	59.844660
2279.242870	85370.589064	59.849665
2279.024434	85211.545381	59.854669
2278.176243	85076.804003	59.859674
2277.537844	84933.745551	59.864679
2277.029136	84780.785557	59.869684
2276.279257	84631.908936	59.874689
2275.575064	84478.094726	59.879693
2274.857010	84319.079924	59.884698
2274.108515	84172.494518	59.889703
2273.714552	84026.056738	59.894708
2272.735234	83882.869309	59.899713
2272.171923	83725.311283	59.904718
2271.640438	83573.827796	59.909722
2270.940209	83421.541851	59.914727
2270.109708	83281.307547	59.919732
2269.605986	83127.712255	59.924737
2269.087673	82972.516862	59.929742
2268.125343	82835.475492	59.934746
2267.449953	82675.540991	59.939751
2267.268456	82524.225067	59.944756
2266.121480	82381.175879	59.949761
2265.538434	82224.868144	59.954766
2265.019325	82090.252152	59.959770
2264.080729	81929.782017	59.964775
2263.501501	81783.306881	59.969780
2262.834102	81632.524453	59.974785
2262.292012	81480.956389	59.979790
2261.476146	81344.852227	59.984794
2261.386166	81184.684212	59.989799
2260.694835	81045.222372	59.994804
2259.386710	80896.219998	59.999809
2258.949906	80729.918790	60.004814
2258.063405	80594.172973	60.009818
2257.812486	80429.517763	60.014823
2256.935870	80291.288135	60.019828
2256.155410	80134.666201	60.024833
2255.636169	79982.224594	60.029838
2254.939422	79838.544841	60.034842
2254.351917	79692.206195	60.039847
2253.741932	79535.631481	60.044852
2253.135966	79396.059498	60.049857
2252.650195	79232.236869	60.054862
2251.951769	79089.259675	60.059866
2251.238633	78933.010077	60.064871
2250.322457	78794.898156	60.069876
2249.704699	78631.418092	60.074881
2249.426869	78482.618298	60.079886
2248.395872	78340.681258	60.084890
2247.795962	78182.619806	60.089895
2247.365876	78027.428461	60.094900
2246.617404	77876.724363	60.099905
2246.279600	77712.117359	60.104910
2245.456511	77563.423401	60.109914
2244.883570	77400.712778	60.114919
2243.972300	77258.365085	60.119924
2243.225475	77105.822549	60.124929
2242.700598	76945.173577	60.129934
2241.758659	76796.288642	60.134938
2241.131629	76646.309390	60.139943
2240.270894	76482.340177	60.144948
2239.601553	76350.313674	60.149953
2238.992361	76195.785636	60.154958
2238.375867	76042.343384	60.159962
2237.779121	75898.288995	60.164967
2237.222359	75742.945102	60.169972
2236.905962	75605.222227	60.174977
2236.351987	75440.047020	60.179982
2235.419169	75297.387067	60.184986
2234.902355	75133.938129	60.189991
2234.352556	74983.040296	60.194996
2233.426681	74814.913437	60.200001
2232.905207	74659.787706	60.205006
2232.014606	74517.462374	60.210010
2231.550259	74344.413274	60.215015
2230.560719	74195.428377	60.220020
2230.029653	74047.372857	60.225025
2229.655266	73887.129828	60.230030
2228.739581	73740.429978	60.235034
2228.273690	73588.458674	60.240039
2227.602822	73430.160551	60.245044
2226.796731	73277.130588	60.250049
2226.156169	73109.733009	60.255054
2225.427485	72964.821025	60.260058
2224.728591	72810.960425	60.265063
2223.993994	72656.308482	60.270068
2222.968132	72511.928382	60.275073
2222.799457	72356.308471	60.280078
2222.005276	72196.513031	60.285082
2221.436026	72049.612326	60.290087
2220.413775	71904.786309	60.295092
2219.904375	71749.554601	60.300097
2219.555898	71600.639478	60.305102
2218.459716	71451.210615	60.310106
2218.049403	71307.419460	60.315111
2217.409644	71145.745679	60.320116
2216.553384	71007.088638	60.325121
2216.298180	70840.998316	60.330126
2215.393029	70698.461932	60.335130
2214.887970	70541.680801	60.340135
2214.186461	70385.647838	60.345140
2213.531630	70231.876326	60.350145
2213.286602	70081.569096	60.355150
2212.039180	69926.855174	60.360154
2211.675822	69774.333156	60.365159
2210.810102	69613.898595	60.370164
2209.783606	69467.539374	60.375169
2209.608395	69305.648703	60.380174
2208.811613	69152.433883	60.385178
2208.501609	68998.927709	60.390183
2207.824714	68843.086807	60.395188
2206.998014	68697.176695	60.400193
2206.240090	68537.506579	60.405198
2205.713160	68387.111409	60.410202
2205.088970	68223.166533	60.415207
2204.422473	68081.542385	60.420212
2203.631152	67923.852297	60.425217
2203.063476	67750.389723	60.430222
2202.500869	67605.427579	60.435226
2201.732282	67442.626851	60.440231
2200.953885	67290.956414	60.445236
2200.417585	67145.442554	60.450241
2199.944281	66978.080218	60.455246
2199.049838	66840.098477	60.460250
2198.454747	66658.318953	60.465255
2197.763932	66516.181308	60.470260
2196.962414	66354.056762	60.475265
2196.457213	66211.971080	60.480270
2195.583609	66058.048786	60.485274
2195.281249	65906.123744	60.490279
2194.670529	65743.692270	60.495284
2193.957389	65600.491543	60.500289
2193.470134	65426.872443	60.505294
2192.551635	65278.643817	60.510298
2192.061816	65114.533042	60.515303
2191.533240	64954.890993	60.520308
2190.503002	64802.618378	60.525313
2190.128617	64628.260392	60.530318
2189.496792	64468.540629	60.535322
2188.723943	64307.970730	60.540327
2187.976505	64151.314575	60.545332
2187.410637	63990.211116	60.550337
2186.566415	63817.448429	60.555342
2185.461566	63669.157378	60.560346
2185.017030	63524.416265	60.565351
2184.646474	63362.375344	60.570356
2183.780147	63216.899330	60.575361
2183.095560	63054.863357	60.580366
2182.379994	62904.851275	60.585370
2181.564665	62745.738609	60.590375
2180.946374	62592.402112	60.595380
2180.301625	62441.122481	60.600385
2179.858461	62294.335948	60.605390
2179.067891	62135.151680	60.610394
2178.753284	61978.793039	60.615399
2177.756868	61821.594140	60.620404
2177.121265	61663.345306	60.625409
2176.744975	61512.530707	60.630414
2176.156274	61363.666196	60.635418
2175.251140	61196.651012	60.640423
2174.395894	61054.450442	60.645428
2173.752440	60886.301229	60.650433
2173.587678	60723.044247	60.655438
2172.430273	60587.232463	60.660442
2171.818426	60432.320303	60.665447
2171.425463	60258.163800	60.670452
2170.483497	60111.470263	60.675457
2170.144378	59955.505863	60.680462
2169.719834	59789.927366	60.685466
2169.110231	59635.379134	60.690471
2168.142757	59486.836515	60.695476
2167.338165	59327.203506	60.700481
2167.134560	59153.609672	60.705486
2165.869909	59002.066784	60.710490
2165.419997	58840.036279	60.715495
2164.717938	58694.050164	60.720500
2164.161627	58538.610013	60.725505
2163.711166	58374.304769	60.730510
2162.715702	58219.607953	60.735514
2162.189870	58060.400545	60.740519
2161.657172	57899.128842	60.745524
2160.610241	57750.115818	60.750529
2160.192732	57581.422544	60.755534
2159.672186	57418.589615	60.760538
2158.900453	57263.507671	60.765543
2158.285611	57098.910680	60.770548
2157.526310	56937.477603	60.775553
2157.187850	56789.936043	60.780558
2156.312973	56634.046576	60.785562
2155.930149	56465.199772	60.790567
2155.124840	56309.283035	60.795572
2153.990556	56149.321506	60.800577
2153.791432	55970.861029	60.805582
2152.863201	55819.790926	60.810586
2152.276290	55669.661619	60.815591
2151.375088	55508.206654	60.820596
2150.879658	55352.274218	60.825601
2150.410119	55179.560582	60.830606
2149.201096	55024.434015	60.835610
2148.853754	54861.716536	60.840615
2148.208636	54720.015478	60.845620
2147.599355	54564.544526	60.850625
2147.211061	54400.919968	60.855630
2146.477434	54233.744269	60.860634
2145.863876	54067.313667	60.865639
2145.085506	53911.213772	60.870644
2144.551995	53758.167893	60.875649
2143.613422	53603.557963	60.880654
2142.797708	53436.114680	60.885658
2142.109970	53273.016092	60.890663
2141.529394	53119.612858	60.895668
2140.844759	52978.630942	60.900673
2140.229540	52816.012249	60.905678
2139.611328	52646.089579	60.910682
2138.993847	52496.260270	60.915687
2138.399066	52340.094176	60.920692
2137.802344	52168.796229	60.925697
2137.158510	52016.522972	60.930702
2136.302209	51854.546024	60.935706
2135.806120	51701.593890	60.940711
2135.075523	51541.165972	60.945716
2134.117204	51374.207398	60.950721
2133.867783	51220.293212	60.955726
2132.915026	51071.104783	60.960730
2132.149745	50907.157207	60.965735
2131.701106	50759.634651	60.970740
2130.876283	50599.894496	60.975745
2130.365128	50437.394704	60.980750
2129.689470	50280.424136	60.985754
2129.007372	50120.751042	60.990759
2128.439479	49963.823107	60.995764
2127.487063	49810.447011	61.000769
2127.480291	49652.306556	61.005774
2126.622676	49481.214894	61.010778
2126.033276	49331.961209	61.015783
2125.280137	49157.793798	61.020788
2124.457417	49004.913392	61.025793
2123.937780	48832.252734	61.030798
2123.161823	48690.809744	61.035802
2122.510587	48519.966654	61.040807
2122.049258	48363.064414	61.045812
2120.763109	48217.422976	61.050817
2120.217817	48040.032291	61.055822
2119.558449	47893.379896	61.060826
2119.133530	47738.049565	61.065831
2118.546829	47579.782341	61.070836
2117.760054	47417.391864	61.075841
2117.305514	47257.091626	61.080846
2116.267057	47108.949625	61.085850
2115.607007	46949.655868	61.090855
2115.368194	46800.940438	61.095860
2114.457046	46632.573435	61.100865
2113.894838	46472.762390	61.105870
2113.096823	46309.378089	61.110874
2112.555144	46166.463212	61.115879
2112.121190	45998.067708	61.120884
2111.399561	45848.601933	61.125889
2110.797326	45684.645216	61.130894
2109.661392	45531.594772	61.135898
2109.390051	45366.750386	61.140903
2108.645327	45209.301328	61.145908
2107.739319	45051.303658	61.150913
2107.018008	44890.804869	61.155918
2106.331653	44739.046858	61.160922
2106.051774	44575.934965	61.165927
2105.565747	44417.930173	61.170932
2104.587889	44261.020043	61.175937
2104.164489	44102.239670	61.180942
2103.278227	43942.424128	61.185946
2102.917124	43776.508464	61.190951
2102.183740	43616.902530	61.195956
2101.228038	43459.496460	61.200961
2100.862725	43294.987043	61.205966
2100.101484	43143.956915	61.210970
2099.408841	42980.606098	61.215975
2098.634254	42821.146859	61.220980
2097.797914	42666.771246	61.225985
2097.393976	42500.355992	61.230990
2096.703440	42354.403345	61.235994
2095.743075	42194.786475	61.240999
2095.267229	42032.023715	61.246004
2094.681455	41882.526270	61.251009
2094.010453	41712.609878	61.256014
2093.399953	41564.444059	61.261018
2093.050337	41394.267963	61.266023
2092.270012	41247.934206	61.271028
2091.604193	41078.288882	61.276033
2090.946874	40911.350555	61.281038
2090.038218	40765.063417	61.286042
2089.292881	40593.789706	61.291047
2089.024450	40427.746137	61.296052
2088.122849	40280.763243	61.301057
2087.428121	40121.934545	61.306062
2086.892810	39957.732236	61.311066
2086.009645	39796.550874	61.316071
2085.334646	39635.889736	61.321076
2084.863780	39473.133117	61.326081
2084.523278	39318.481353	61.331086
2083.596244	39158.372164	61.336090
2083.154304	39003.518042	61.341095
2082.235625	38833.258569	61.346100
2081.451813	38679.239403	61.351105
2081.044243	38510.331110	61.356110
2080.285519	38357.566021	61.361114
2079.558593	38197.130650	61.366119
2079.097664	38036.181958	61.371124
2078.257445	37875.448307	61.376129
2077.841656	37705.306908	61.381134
2077.102190	37553.927555	61.386138
2076.160747	37387.705922	61.391143
2075.921833	37215.007588	61.396148
2075.265959	37059.112972	61.401153
2074.561494	36893.980861	61.406158
2073.626386	36733.146705	61.411162
2073.430647	36569.808498	61.416167
2072.902578	36402.220696	61.421172
2071.850739	36239.462517	61.426177
2071.258571	36068.075908	61.431182
2070.513686	35904.415621	61.436186
2069.945006	35743.556515	61.441191
2069.527375	35579.997621	61.446196
2068.512929	35414.211711	61.451201
2068.202037	35243.444811	61.456206
2067.460693	35092.519412	61.461210
2066.763889	34909.628706	61.466215
2065.989806	34742.284627	61.471220
2064.950218	34591.589671	61.476225
2064.514952	34427.994283	61.481230
2063.715226	34260.900909	61.486234
2063.042787	34100.938559	61.491239
2062.457003	33926.807283	61.496244
2062.076959	33766.155400	61.501249
2061.209565	33605.054575	61.506254
2060.357175	33446.149546	61.511258
2059.774007	33274.932440	61.516263
2059.352253	33110.832705	61.521268
2058.154846	32968.853179	61.526273
2057.594167	32795.975031	61.531278
2056.829408	32634.537094	61.536282
2056.290838	32478.628743	61.541287
2055.700151	32326.314004	61.546292
2054.790736	32162.302645	61.551297
2054.187714	32000.655623	61.556302
2053.468559	31851.140418	61.561306
2053.158027	31684.889786	61.566311
2052.618971	31538.469596	61.571316
2051.830247	31385.363840	61.576321
2051.014414	31212.917261	61.581326
2050.373858	31052.732864	61.586330
2049.797473	30884.405740	61.591335
2049.292861	30735.656665	61.596340
2048.571500	30574.582818	61.601345
2048.078860	30410.197329	61.606350
2047.042115	30257.315261	61.611354
2046.295965	30094.580021	61.616359
2045.666601	29933.053918	61.621364
2044.777350	29782.841978	61.626369
2044.319811	29625.097745	61.631374
2043.942153	29472.150043	61.636378
2043.122415	29313.184989	61.641383
2042.266250	29140.280052	61.646388
2041.491419	28988.038190	61.651393
2041.358972	28833.566176	61.656398
2040.449334	28681.283803	61.661402
2039.780537	28516.648339	61.666407
2039.319207	28350.357582	61.671412
2038.303107	28201.820205	61.676417
2037.811029	28032.921445	61.681422
2037.275139	27879.955376	61.686426
2036.337985	27727.059165	61.691431
2035.742108	27570.320470	61.696436
2035.029699	27418.866188	61.701441
2034.600667	27257.237738	61.706446
2033.500893	27103.501237	61.711450
2032.860720	26945.388670	61.716455
2032.642099	26786.353797	61.721460
2031.611992	26649.788521	61.726465
2031.223951	26472.162050	61.731470
2030.741305	26327.639793	61.736474
2030.112713	26157.612604	61.741479
2029.350398	26001.486590	61.746484
2028.655453	25844.811981	61.751489
2027.965144	25676.759910	61.756494
2027.020103	25529.082513	61.761498
2026.607676	25370.995087	61.766503
2025.878964	25193.887757	61.771508
2024.801098	25048.813606	61.776513
2024.488671	24899.907553	61.781518
2023.657847	24741.144861	61.786522
2022.873235	24585.862231	61.791527
2022.341531	24432.275972	61.796532
2021.653968	24284.413635	61.801537
2021.036705	24132.178440	61.806542
2020.336894	23978.597955	61.811546
2019.745145	23828.820699	61.816551
2019.545041	23671.050429	61.821556
2018.384651	23525.306739	61.826561
2017.972144	23359.922975	61.831566
2017.350649	23209.772493	61.836570
2016.700026	23055.187891	61.841575
2015.899806	22891.869113	61.846580
2014.917886	22746.045033	61.851585
2014.462526	22590.186363	61.856590
2013.545758	22447.795063	61.861594
2012.649948	22288.606028	61.866599
2012.355284	22143.359864	61.871604
2011.559759	21994.149447	61.876609
2010.881233	21853.248812	61.881614
2010.161371	21690.916653	61.886618
2009.827273	21550.009859	61.891623
2008.962549	21394.828007	61.896628
2008.088903	21253.175714	61.901633
2007.792026	21092.001662	61.906638
2006.973315	20948.081350	61.911642
2006.149499	20803.809060	61.916647
2005.677115	20652.632026	61.921652
2004.674563	20497.105085	61.926657
2003.989424	20363.175248	61.931662
2003.503293	20226.616327	61.936666
2002.412119	20065.288316	61.941671
2002.022514	19926.328473	61.946676
2001.564983	19797.508876	61.951681
2000.906538	19641.221731	61.956686
1999.773112	19504.098016	61.961690
1999.096970	19374.016742	61.966695
1998.963445	19218.187350	61.971700
1997.819413	19077.239045	61.976705
1996.711103	18935.729398	61.981710
1996.148408	18807.507777	61.986714
1995.731073	18670.127751	61.991719
1994.801849	18544.970212	61.996724
1993.560072	18427.652396	62.001729
1993.377113	18283.850669	62.006734
1992.249984	18160.957297	62.011738
1991.107017	18062.075570	62.016743
1990.421418	17940.175605	62.021748
1989.299648	17847.183862	62.026753
1988.351476	17735.868573	62.031758
1987.482620	17648.210771	62.036762
1986.044657	17564.891959	62.041767
1985.031136	17480.406457	62.046772
1983.814382	17407.503959	62.051777
1983.138327	17332.220352	62.056782
1982.193168	17280.536643	62.061786
1981.451697	17220.331523	62.066791
1980.811524	17153.582076	62.071796
1979.993598	17083.469719	62.076801
1979.303624	17032.418861	62.081806
1978.482113	16988.919326	62.086810
1977.870070	16933.112115	62.091815
1977.688117	16886.823680	62.096820
1976.336931	16837.167783	62.101825
1976.317520	16776.823747	62.106830
1975.673726	16726.804732	62.111834
1974.927940	16680.044404	62.116839
1974.742394	16623.020781	62.121844
1973.830966	16551.450443	62.126849
1973.564170	16507.967035	62.131854
1972.971906	16455.844899	62.136858
1972.003044	16391.006979	62.141863
1971.756446	16328.131360	62.146868
1970.766017	16287.269661	62.151873
1970.367815	16210.068099	62.156878
1969.684691	16164.904427	62.161882
1968.791900	16094.408671	62.166887
1968.087024	16051.088427	62.171892
1967.430153	15991.065294	62.176897
1966.868154	15931.103306	62.181902
1966.036073	15878.838762	62.186906
1965.469564	15824.475388	62.191911
1964.889431	15762.121774	62.196916
1964.120115	15711.267449	62.201921
1963.832730	15652.323942	62.206926
1963.146011	15602.076445	62.211930
1962.621821	15540.259150	62.216935
1961.873911	15481.268831	62.221940
1961.264553	15430.229237	62.226945
1960.916821	15356.286246	62.231950
1960.313139	15312.216639	62.236954
1959.738522	15248.388531	62.241959
1959.319046	15179.201460	62.246964
1958.271721	15118.243834	62.251969
1957.593520	15043.307772	62.256974
1956.819908	14993.427075	62.261978
1956.178360	14928.949343	62.266983
1955.507806	14861.119502	62.271988
1954.636200	14803.493606	62.276993
1953.988837	14748.467254	62.281998
1953.405625	14693.972620	62.287002
1952.602087	14639.674372	62.292007
1951.926956	14570.093103	62.297012
1951.475035	14533.921214	62.302017
1951.022955	14469.982687	62.307022
1950.204628	14402.013786	62.312026
1949.694639	14331.835512	62.317031
1949.203235	14285.784153	62.322036
1948.430763	14226.782146	62.327041
1947.674276	14160.373327	62.332046
1946.818623	14100.443208	62.337050
1946.076905	14049.638065	62.342055
1945.781395	13994.980499	62.347060
1944.952085	13930.011382	62.352065
1944.086049	13874.013033	62.357070
1943.562732	13812.862399	62.362074
1943.082454	13749.369651	62.367079
1942.658814	13699.647748	62.372084
1941.419807	13638.040078	62.377089
1941.300752	13573.717739	62.382094
1940.542956	13511.845788	62.387098
1939.983321	13451.597100	62.392103
1939.322037	13387.902477	62.397108
1938.385344	13342.548075	62.402113
1938.034251	13279.401071	62.407118
1936.972750	13227.737667	62.412122
1936.627995	13156.238063	62.417127
1935.886771	13104.151769	62.422132
1935.430803	13049.303384	62.427137
1934.838507	12985.675251	62.432142
1934.126054	12927.354802	62.437146
1933.140128	12865.788908	62.442151
1932.796378	12791.539965	62.447156
1932.091682	12755.713666	62.452161
1931.796665	12676.712177	62.457166
1930.906528	12614.424064	62.462170
1930.101801	12546.582709	62.467175
1929.518077	12471.872136	62.472180
1928.612921	12431.740909	62.477185
1928.323763	12352.589850	62.482190
1927.316113	12310.315252	62.487194
1926.510284	12244.800102	62.492199
1925.821308	12183.962562	62.497204
1924.972001	12135.796829	62.502209
1924.544908	12068.997066	62.507214
1923.846579	12016.746528	62.512218
1923.414217	11964.159627	62.517223
1922.569452	11902.913755	62.522228
1922.087343	11852.274489	62.527233
1921.540534	11793.876872	62.532238
1920.650982	11726.454489	62.537242
1919.920087	11668.194285	62.542247
1919.356741	11606.863122	62.547252
1918.813708	11547.741104	62.552257
1918.620857	11483.881486	62.557262
1917.535674	11440.958825	62.562266
1916.881772	11367.502663	62.567271
1916.579335	11316.604691	62.572276
1915.260515	11249.980863	62.577281
1915.280265	11188.836975	62.582286
1914.131730	11134.292061	62.587290
1913.488809	11068.493598	62.592295
1913.334899	11006.006282	62.597300
1912.426131	10956.584005	62.602305
1911.404111	10878.398084	62.607310
1910.797882	10821.119080	62.612314
1910.398690	10760.656887	62.617319
1909.667954	10704.112151	62.622324
1908.570952	10635.031197	62.627329
1908.201318	10575.842066	62.632334
1907.588768	10522.563491	62.637338
1906.784159	10465.968650	62.642343
1906.435215	10409.660685	62.647348
1905.506895	10350.115341	62.652353
1904.832611	10292.079094	62.657358
1904.036496	10232.596469	62.662362
1903.417283	10170.155312	62.667367
1903.123049	10113.724972	62.672372
1902.173375	10055.457604	62.677377
1901.759029	9996.844334	62.682382
1901.020375	9928.727127	62.687386
1900.107762	9882.773570	62.692391
1900.006148	9820.722322	62.697396
1899.155114	9749.920371	62.702401
1898.418542	9695.472292	62.707406
1897.787537	9642.227776	62.712410
1896.941606	9578.028220	62.717415
1896.865525	9518.981657	62.722420
1895.562661	9465.197088	62.727425
1895.018778	9399.430834	62.732430
1894.583806	9339.129935	62.737434
1893.795676	9280.710548	62.742439
1893.311679	9220.035670	62.747444
1892.415064	9162.368465	62.752449
1891.654969	9100.068126	62.757454
1891.130082	9042.254015	62.762458
1890.684897	8988.116480	62.767463
1889.980085	8914.238583	62.772468
1888.913722	8864.938747	62.777473
1888.759402	8800.016593	62.782478
1888.091315	8735.839752	62.787482
1887.244264	8685.254483	62.792487
1886.602916	8617.902891	62.797492
1885.742432	8561.556839	62.802497
1885.313303	8493.075154	62.807502
1884.640190	8428.452337	62.812506
1883.927111	8381.461542	62.817511
1883.307662	8317.662178	62.822516
1882.573040	8257.907836	62.827521
1882.112828	8198.589023	62.832526
1881.324896	8144.343682	62.837530
1880.402309	8075.763959	62.842535
1880.033571	8022.811747	62.847540
1879.134317	7964.308258	62.852545
1878.829442	7907.294686	62.857550
1878.254189	7841.891308	62.862554
1877.293003	7787.658994	62.867559
1877.054161	7730.140212	62.872564
1875.923790	7667.250277	62.877569
1874.984041	7599.850074	62.882574
1874.306328	7544.146617	62.887578
1873.911563	7480.268626	62.892583
1873.148694	7426.694017	62.897588
1872.547910	7367.664300	62.902593
1871.980428	7301.105628	62.907598
1871.273085	7246.154229	62.912602
1870.463374	7191.414913	62.917607
1869.739356	7132.504297	62.922612
1869.067747	7076.925468	62.927617
1868.711163	7019.918769	62.932622
1867.934259	6968.993740	62.937626
1867.341682	6908.142379	62.942631
1866.694371	6846.870844	62.947636
1865.732891	6795.703573	62.952641
1865.404303	6739.214120	62.957646
1864.851647	6675.124068	62.962650
1864.066658	6622.799024	62.967655
1863.489208	6553.363017	62.972660
1862.535588	6507.118363	62.977665
1862.112217	6445.587340	62.982670
1861.539873	6383.979258	62.987674
1860.631613	6332.476216	62.992679
1860.214613	6270.631761	62.997684
1859.462567	6207.625250	63.002689
1859.134725	6146.921925	63.007694
1858.189295	6095.779768	63.012698
1857.305833	6038.461368	63.017703
1856.900114	5962.652869	63.022708
1856.092541	5914.765975	63.027713
1855.634014	5853.042649	63.032718
1854.696189	5797.260061	63.037722
1854.256999	5736.725170	63.042727
1853.616319	5675.460584	63.047732
1852.363192	5625.343011	63.052737
1852.315585	5554.312393	63.057742
1851.654385	5503.628015	63.062746
1850.751917	5448.430320	63.067751
1850.614125	5379.075938	63.072756
1849.645541	5328.280851	63.077761
1848.886352	5270.593930	63.082766
1848.335596	5216.796464	63.087770
1847.478930	5151.322647	63.092775
1847.013645	5093.669419	63.097780
1845.887071	5041.597443	63.102785
1845.436791	4974.901271	63.107790
1844.730159	4919.095555	63.112794
1844.264208	4865.576941	63.117799
1843.627903	4802.736299	63.122804
1842.989192	4754.119693	63.127809
1842.318716	4683.356200	63.132814
1841.628522	4637.499121	63.137818
1841.110921	4571.453514	63.142823
1840.371172	4514.242050	63.147828
1839.616285	4453.852455	63.152833
1839.234330	4401.212616	63.157838
1838.398870	4340.395407	63.162842
1837.463361	4290.621569	63.167847
1837.065043	4228.579224	63.172852
1836.189326	4171.563401	63.177857
1835.654246	4114.621481	63.182862
1834.767306	4045.395466	63.187866
1834.382688	3999.301009	63.192871
1833.476902	3938.119654	63.197876
1832.614999	3883.220297	63.202881
1832.409765	3815.342198	63.207886
1831.636684	3764.556182	63.212890
1831.161714	3720.424112	63.217895
1830.500527	3654.961416	63.222900
1829.541328	3589.554213	63.227905
1828.933879	3545.293075	63.232910
1828.283680	3483.722096	63.237914
1827.764137	3437.493101	63.242919
1827.300355	3372.700625	63.247924
1826.058765	3323.521245	63.252929
1825.792441	3268.623480	63.257934
1824.980685	3212.445058	63.262938
1823.972673	3153.898262	63.267943
1823.396946	3104.522422	63.272948
1822.827167	3046.758965	63.277953
1822.484489	2985.678298	63.282958
1821.606789	2943.633704	63.287962
1820.584017	2888.213181	63.292967
1819.902176	2824.281841	63.297972
1819.486360	2777.022754	63.302977
1819.079971	2726.055161	63.307982
1818.515909	2673.340037	63.312986
1817.612184	2621.021278	63.317991
1816.913340	2562.977409	63.322996
1815.949897	2509.749835	63.328001
1815.813346	2459.729994	63.333006
1814.884604	2410.522162	63.338010
1814.509952	2350.664416	63.343015
1813.783501	2299.033111	63.348020
1812.826776	2243.123529	63.353025
1812.163173	2194.526472	63.358030
1811.708689	2144.959568	63.363034
1811.024576	2092.003804	63.368039
1810.537887	2043.983194	63.373044
1809.478875	1989.508646	63.378049
1809.300272	1923.627756	63.383054
1808.290076	1881.633290	63.388058
1807.422887	1828.782466	63.393063
1806.875105	1768.266992	63.398068
1806.032178	1724.679597	63.403073
1805.607293	1683.150266	63.408078
1805.128359	1617.814432	63.413082
1804.078963	1572.464006	63.418087
1803.522836	1514.668179	63.423092
1802.801446	1469.762763	63.428097
1802.255139	1417.613158	63.433102
1801.684631	1367.938794	63.438106
1800.737783	1318.961473	63.443111
1800.477072	1261.864102	63.448116
1799.523439	1218.828839	63.453121
1798.912334	1174.105532	63.458126
1798.126729	1114.622482	63.463130
1797.042431	1070.636971	63.468135
1796.854049	1027.065231	63.473140
1796.175860	988.880336	63.478145
1795.674738	934.836055	63.483150
1794.865870	895.708616	63.488154
1794.484760	838.890650	63.493159
1793.729486	786.338095	63.498164
1792.734422	747.710558	63.503169
1791.960138	696.000296	63.508174
1791.179697	661.708669	63.513178
1790.763140	614.474070	63.518183
1790.203179	569.414927	63.523188
1789.537073	524.164622	63.528193
1788.701272	464.977638	63.533198
1788.283689	434.853543	63.538202
1787.034350	391.757311	63.543207
1786.658952	344.972788	63.548212
1785.765946	311.562443	63.553217
1785.273347	262.696341	63.558222
1784.500260	224.161115	63.563226
1783.886295	186.988401	63.568231
1783.033013	142.530657	63.573236
1782.110793	111.769877	63.578241
1781.643849	65.705667	63.583246
1780.991371	46.498660	63.588250
1779.929078	20.981398	63.593255
1779.574339	-23.504534	63.598260
1778.301126	-37.762373	63.603265
1775.911920	-26.463105	63.608270
1772.999709	27.655958	63.613274
1772.612499	34.261516	63.618279
1773.495886	24.713521	63.623284
1773.173321	37.181144	63.628289
1773.170840	42.077765	63.633294
1773.289043	28.228099	63.638298
1771.702075	42.501773	63.643303
1770.738776	40.530656	63.648308
1769.921519	46.666789	63.653313
1769.681530	40.947664	63.658318
1768.793305	50.192077	63.663322
1768.105388	49.962271	63.668327
1768.289897	45.665899	63.673332
1767.523549	48.037799	63.678337
1766.930504	50.768518	63.683342
1765.775373	52.328559	63.688346
1765.076281	47.918616	63.693351
1765.045123	45.296456	63.698356
1763.840507	50.376087	63.703361
1763.195384	54.960038	63.708366
1762.248765	55.154498	63.713370
1761.529117	53.947330	63.718375
1760.873409	51.588340	63.723380
1760.493761	52.380292	63.728385
1760.571020	58.907376	63.733390
1759.775775	54.779196	63.738394
1758.337261	55.679370	63.743399
1758.073626	60.333627	63.748404
1757.653702	61.250243	63.753409
1756.968929	53.854550	63.758414
1756.416623	52.108321	63.763418
1755.141120	62.149074	63.768423
1754.882681	50.238852	63.773428
1754.292509	64.236000	63.778433
1753.805202	52.901417	63.783438
1752.481090	58.316986	63.788442
1752.272739	50.698991	63.793447
1751.912214	50.521274	63.798452
1750.352049	63.081373	63.803457
1750.185987	61.005738	63.808462
1750.134914	59.971512	63.813466
1748.877342	54.117522	63.818471
1748.332162	58.404920	63.823476
1747.250337	62.861114	63.828481
1747.060116	49.539783	63.833486
1746.780468	52.384736	63.838490
1745.318771	52.566383	63.843495
1744.930733	56.190187	63.848500
1744.327787	59.772428	63.853505
1743.704733	50.941432	63.858510
1742.767845	60.207778	63.863514
1742.406050	59.505159	63.868519
1741.686211	61.847606	63.873524
1740.696738	56.964985	63.878529
1740.686559	59.231004	63.883534
1740.121836	68.316834	63.888538
1738.874684	57.377297	63.893543
1738.156150	62.742436	63.898548
1737.556839	57.752127	63.903553
1737.256646	55.710409	63.908558
1736.537234	50.611447	63.913562
1735.395641	60.001762	63.918567
1735.385797	51.196385	63.923572
1734.390964	58.852469	63.928577
1733.525377	54.639278	63.933582
1733.204118	58.427514	63.938586
1732.848321	61.724514	63.943591
1732.029860	45.159952	63.948596
1731.388278	62.621804	63.953601
1730.715247	60.621949	63.958606
1730.352913	50.218394	63.963610
1729.309125	61.882822	63.968615
1728.993573	51.445030	63.973620
1727.920674	64.353519	63.978625
1727.112852	53.462490	63.983630
1726.546699	56.717206	63.988634
1725.383674	61.419682	63.993639
1725.328258	50.202595	63.998644
1724.665233	61.049650	64.003649
1723.970499	59.048513	64.008654
1723.496799	45.901515	64.013658
1722.479920	65.338890	64.018663
1722.443809	46.000911	64.023668
1721.568360	58.706159	64.028673
1721.113061	43.168831	64.033678
1720.528737	60.944850	64.038682
1719.618896	63.639163	64.043687
1718.791006	63.964587	64.048692
1717.851826	57.689479	64.053697
1717.428430	59.699436	64.058702
1717.029545	55.640783	64.063706
1716.442777	55.396504	64.068711
1715.865648	61.056145	64.073716
1714.792588	55.095602	64.078721
1713.472975	57.977990	64.083726
1713.471975	56.279828	64.088730
1713.020647	57.135208	64.093735
1711.970279	55.971115	64.098740
1711.041429	53.999279	64.103745
1710.826389	55.990339	64.108750
1710.415165	56.986001	64.113754
1709.693054	56.186076	64.118759
1709.087287	56.192387	64.123764
1708.452643	53.356999	64.128769
1707.942540	60.652269	64.133774
1706.800465	52.484008	64.138778
1705.792590	67.780627	64.143783
1705.215739	52.581131	64.148788
1704.602748	66.668637	64.153793
1704.484476	66.824599	64.158798
1703.654907	59.265845	64.163802
1702.889150	68.730522	64.168807
1702.579899	57.536401	64.173812
1702.127244	69.775562	64.178817
1701.490915	56.491970	64.183822
1700.423257	64.260553	64.188826
1699.431185	60.029617	64.193831
1698.763321	63.481835	64.198836
1698.265178	64.513380	64.203841
1697.710074	52.446867	64.208846
1697.318510	56.640493	64.213850
1696.611265	65.725308	64.218855
1696.246274	66.317830	64.223860
1695.015140	58.416019	64.228865
1694.219453	60.491415	64.233870
1693.708289	62.017018	64.238874
1693.088852	61.096716	64.243879
1692.725134	60.394410	64.248884
1692.070315	73.950848	64.253889
1690.989943	67.542059	64.258894
1690.002900	73.809263	64.263898
1689.396512	66.809552	64.268903
1689.317897	57.218770	64.273908
1688.468779	73.825810	64.278913
1687.364720	59.241458	64.283918
1687.627128	68.460844	64.288922
1686.283747	66.118054	64.293927
1686.345117	60.001003	64.298932
1685.986629	63.205399	64.303937
1684.772336	65.954385	64.308942
1683.515442	61.205720	64.313946
1682.917636	66.715694	64.318951
1682.978479	53.319807	64.323956
1682.316232	70.742377	64.328961
1681.127416	57.924994	64.333966
1680.362793	65.233886	64.338970
1679.344077	62.453198	64.343975
1679.278553	60.369485	64.348980
1678.449112	54.707721	64.353985
1678.037650	61.178384	64.358990
1677.480071	59.817770	64.363994
1677.074963	58.527553	64.368999
1676.118637	56.295177	64.374004
1675.176339	64.498002	64.379009
1674.399390	58.230260	64.384014
1674.071284	64.522112	64.389018
1673.459773	59.177381	64.394023
1672.982248	56.436891	64.399028
1672.159432	68.747460	64.404033
1671.192269	51.927429	64.409038
1670.433557	68.997904	64.414042
1669.558104	60.456164	64.419047
1669.284555	60.502755	64.424052
1668.711849	52.920567	64.429057
1668.223552	55.967393	64.434062
1667.872794	47.529974	64.439066
1667.171714	67.372924	64.444071
1666.325180	59.146701	64.449076
1665.500578	60.556520	64.454081
1664.670117	61.533625	64.459086
1664.467233	59.501690	64.464090
1663.235306	62.543634	64.469095
1662.747650	47.255878	64.474100
1661.663000	65.064065	64.479105
1660.943681	57.929347	64.484110
1660.779880	56.936683	64.489114
1660.089434	68.794162	64.494119
1659.915769	52.313285	64.499124
1659.346587	69.885070	64.504129
1658.413709	52.184426	64.509134
1657.507957	59.230320	64.514138
1656.828129	66.204064	64.519143
1656.590043	57.898550	64.524148
1655.773878	62.139123	64.529153
1654.971656	55.200495	64.534158
1653.975436	55.259376	64.539162
1653.154680	65.857118	64.544167
1652.774740	55.732330	64.549172
1652.040120	61.913717	64.554177
1651.511732	59.957139	64.559182
1651.068500	58.163648	64.564186
1650.604577	67.227168	64.569191
1649.872003	56.660095	64.574196
1648.802941	65.285169	64.579201
1648.288950	57.061326	64.584206
1647.965391	57.795501	64.589210
1647.146301	70.892352	64.594215
1646.121604	50.213365	64.599220
1645.301111	62.966670	64.604225
1644.583971	58.868700	64.609230
1644.795762	53.982963	64.614234
1643.848279	56.074599	64.619239
1643.637587	62.191690	64.624244
1642.714418	63.476828	64.629249
1641.802149	55.087602	64.634254
1641.390202	62.454018	64.639258
1639.913506	65.288857	64.644263
1639.191602	54.787901	64.649268
1638.804085	65.517094	64.654273
1638.105211	59.877180	64.659278
1638.153800	56.327760	64.664282
1637.202034	66.840665	64.669287
1636.942573	52.469107	64.674292
1636.006210	68.844013	64.679297
1634.933505	61.413789	64.684302
1634.635637	56.181670	64.689306
1634.009845	68.391566	64.694311
1633.324134	54.642780	64.699316
1632.184612	64.646212	64.704321
1631.484838	49.863649	64.709326
1631.223800	59.634500	64.714330
1630.403670	57.065129	64.719335
1629.883423	59.043176	64.724340
1629.625161	67.096360	64.729345
1628.265975	61.600758	64.734350
1627.907071	58.828820	64.739354
1627.360805	61.742942	64.744359
1627.137836	54.207709	64.749364
1625.743711	67.533092	64.754369
1624.707281	58.042426	64.759374
1624.367656	54.016955	64.764378
1623.781653	65.619735	64.769383
1623.480739	58.210419	64.774388
1623.128394	52.349894	64.779393
1622.129403	55.708075	64.784398
1621.038679	58.975178	64.789402
1620.202927	58.433017	64.794407
1619.934546	58.869860	64.799412
1619.288816	57.920638	64.804417
1619.079001	51.586484	64.809422
1618.037612	65.207481	64.814426
1617.382100	59.223232	64.819431
1616.762823	52.362789	64.824436
1616.123673	57.609690	64.829441
1615.143765	61.934630	64.834446
1614.728445	57.143778	64.839450
1613.764620	63.192856	64.844455
1613.420261	52.100527	64.849460
1612.691684	62.475483	64.854465
1612.328674	57.293138	64.859470
1611.687004	57.074949	64.864474
1610.579104	63.515907	64.869479
1610.068513	55.942790	64.874484
1609.410952	55.604129	64.879489
1608.722186	53.499581	64.884494
1607.768364	55.010365	64.889498
1606.991118	51.005531	64.894503
1606.792058	51.997466	64.899508
1605.962097	55.850751	64.904513
1605.725142	42.240428	64.909518
1605.462897	49.564136	64.914522
1604.044343	51.180283	64.919527
1603.370904	50.727457	64.924532
1602.939674	52.090573	64.929537
1602.103391	42.583903	64.934542
1601.535089	56.687962	64.939546
1600.207296	60.539912	64.944551
1599.859630	58.854246	64.949556
1599.297243	62.147810	64.954561
1598.824305	54.084612	64.959566
1598.686859	49.279585	64.964570
1597.790983	59.327895	64.969575
1596.758227	49.552825	64.974580
1595.760588	49.906831	64.979585
1595.425872	54.692230	64.984590
1595.439701	44.187958	64.989594
1594.328668	56.191093	64.994599
1593.874853	51.461553	64.999604
1593.031958	60.127980	65.004609
1592.628104	52.342381	65.009614
1591.846808	50.876984	65.014618
1590.535759	61.779695	65.019623
1590.207812	48.257938	65.024628
1589.665315	48.788790	65.029633
1589.028078	52.565733	65.034638
1588.295597	56.630610	65.039642
1587.146925	59.944777	65.044647
1587.083157	59.612711	65.049652
1586.551121	58.590245	65.054657
1585.969782	60.259474	65.059662
1585.011209	58.030644	65.064666
1584.047254	54.033402	65.069671
1583.533648	67.937980	65.074676
1583.176489	58.971757	65.079681
1582.717645	56.952109	65.084686
1581.777895	55.414121	65.089690
1580.767143	62.140840	65.094695
1580.485481	49.292948	65.099700
1579.922651	63.306262	65.104705
1579.188550	51.276112	65.109710
1578.489651	54.197144	65.114714
1577.748676	50.110868	65.119719
1577.472319	44.752349	65.124724
1576.207221	65.692534	65.129729
1575.152434	55.400598	65.134734
1574.831242	55.908911	65.139738
1574.212314	64.325307	65.144743
1573.900482	58.103554	65.149748
1573.451004	54.973870	65.154753
1572.846475	56.481212	65.159758
1572.081220	57.570983	65.164762
1571.061849	61.323489	65.169767
1570.521966	51.799700	65.174772
1569.625087	53.708287	65.179777
1568.552193	59.752628	65.184782
1567.839829	56.466021	65.189786
1567.554098	58.514050	65.194791
1567.356909	58.619480	65.199796
1566.777539	57.426350	65.204801
1566.271707	63.371143	65.209806
1565.377011	47.116805	65.214810
1564.290617	57.528112	65.219815
1564.119683	52.618026	65.224820
1563.735188	55.974792	65.229825
1562.484306	62.389598	65.234830
1561.680137	46.180802	65.239834
1561.014568	62.665651	65.244839
1560.705900	51.074100	65.249844
1560.131684	48.322191	65.254849
1558.887544	53.259958	65.259854
1558.533172	42.651769	65.264858
1557.518370	58.250696	65.269863
1557.564430	57.872799	65.274868
1557.054389	47.899593	65.279873
1555.941216	59.261289	65.284878
1555.209809	49.547170	65.289882
1554.441470	59.800723	65.294887
1554.066851	48.233846	65.299892
1553.655115	49.461414	65.304897
1552.560808	62.688727	65.309902
1551.773569	48.845728	65.314906
1551.204496	61.320994	65.319911
1550.930791	46.439240	65.324916
1549.919741	58.920071	65.329921
1549.237906	54.827561	65.334926
1548.800914	61.450518	65.339930
1548.120070	57.105549	65.344935
1547.737580	48.802503	65.349940
1546.335259	57.121021	65.354945
1545.521136	51.794330	65.359950
1545.358883	49.281311	65.364954
1544.816819	56.247375	65.369959
1544.645020	61.374310	65.374964
1543.341407	47.405208	65.379969
1542.504784	55.094555	65.384974
1542.165073	58.951967	65.389978
1541.673367	54.797714	65.394983
1540.862646	49.941974	65.399988
1540.059408	61.681771	65.404993
1539.315217	52.849589	65.409998
1539.096067	53.398462	65.415002
1538.335716	57.887230	65.420007
1537.674655	58.397508	65.425012
1536.823954	52.095808	65.430017
1536.519083	67.105735	65.435022
1535.104527	45.107413	65.440026
1533.959662	48.900367	65.445031
1534.001299	53.969735	65.450036
1533.460171	57.721960	65.455041
1533.313250	56.822813	65.460046
1532.813195	53.576599	65.465050
1531.450359	56.904315	65.470055
1530.882097	51.519644	65.475060
1530.482189	48.580781	65.480065
1529.875059	59.275483	65.485070
1529.096960	45.431045	65.490074
1528.297924	54.010094	65.495079
1527.708858	57.205411	65.500084
1526.428030	63.561914	65.505089
1525.734488	52.561356	65.510094
1525.190429	47.772059	65.515098
1524.545917	54.949936	65.520103
1524.104005	44.322549	65.525108
1523.662545	51.007712	65.530113
1523.637853	55.426904	65.535118
1522.749459	48.658134	65.540122
1521.689104	55.485786	65.545127
1521.056181	46.990736	65.550132
1519.971128	57.130619	65.555137
1519.102525	48.333984	65.560142
1518.740847	54.536562	65.565146
1518.180060	53.416182	65.570151
1517.887459	43.069412	65.575156
1517.701486	51.106371	65.580161
1516.261508	46.202395	65.585166
1516.108631	42.566725	65.590170
1515.115014	56.935478	65.595175
1514.569128	64.283764	65.600180
1513.379156	57.876711	65.605185
1512.660903	49.671175	65.610190
1512.376144	52.277271	65.615194
1512.207503	63.846861	65.620199
1511.085036	47.638202	65.625204
1510.003376	57.717628	65.630209
1509.392619	62.873312	65.635214
1509.216869	46.750763	65.640218
1508.501987	59.529885	65.645223
1507.907306	49.644255	65.650228
1507.136249	56.960510	65.655233
1506.603116	46.894799	65.660238
1506.127622	59.938646	65.665242
1504.711231	56.084285	65.670247
1504.101868	48.615202	65.675252
1503.697483	60.021982	65.680257
1503.074423	50.978189	65.685262
1503.001496	50.932998	65.690266
1501.836748	63.536033	65.695271
1501.014349	51.911013	65.700276
1500.199884	58.671220	65.705281
1499.756230	56.385836	65.710286
1499.278148	54.153229	65.715290
1498.680858	47.040184	65.720295
1497.885261	50.049135	65.725300
1497.148545	54.430082	65.730305
1496.714647	48.544698	65.735310
1496.223962	44.328798	65.740314
1495.003035	53.421149	65.745319
1494.846050	48.601892	65.750324
1494.144281	50.927336	65.755329
1492.896483	50.512188	65.760334
1492.488950	49.365886	65.765338
1491.554086	62.440152	65.770343
1491.258032	48.105989	65.775348
1491.006264	46.080265	65.780353
1489.586574	55.522733	65.785358
1489.002089	43.339549	65.790362
1488.086499	57.643872	65.795367
1487.790551	51.224081	65.800372
1487.201697	51.256140	65.805377
1486.690620	53.795703	65.810382
1486.358899	59.399039	65.815386
1485.140910	59.207806	65.820391
1484.553886	44.077828	65.825396
1483.923542	46.201122	65.830401
1483.507494	53.654925	65.835406
1483.213089	44.292426	65.840410
1481.996552	51.868697	65.845415
1481.467754	47.168445	65.850420
1480.757954	59.904187	65.855425
1479.607874	54.285565	65.860430
1479.160581	46.448554	65.865434
1478.530764	56.494035	65.870439
1478.090767	45.670821	65.875444
1477.976797	58.827524	65.880449
1476.865789	55.454488	65.885454
1476.204665	57.123802	65.890458
1475.418785	51.806840	65.895463
1474.638196	46.545808	65.900468
1473.731592	51.718545	65.905473
1473.051234	59.602267	65.910478
1472.791504	52.941766	65.915482
1472.291603	58.475637	65.920487
1471.523081	55.426633	65.925492
1470.819665	44.299944	65.930497
1469.938675	59.081301	65.935502
1469.591290	47.540081	65.940506
1468.925282	54.801805	65.945511
1468.240395	49.114000	65.950516
1467.474740	49.197811	65.955521
1466.502854	52.871846	65.960526
1466.530072	45.640650	65.965530
1465.400079	61.866582	65.970535
1465.091837	49.959612	65.975540
1464.469525	57.413082	65.980545
1463.498159	55.988967	65.985550
1462.939527	53.802283	65.990554
1461.586606	52.446687	65.995559
1461.486870	50.258040	66.000564
1460.937128	55.082350	66.005569
1460.527280	54.485176	66.010574
1459.620491	54.495228	66.015578
1458.626449	67.012808	66.020583
1458.219689	49.342209	66.025588
1457.777281	45.993817	66.030593
1457.004350	50.366336	66.035598
1456.417990	57.361528	66.040602
1455.372306	53.265369	66.045607
1455.348066	43.992402	66.050612
1453.991947	51.314910	66.055617
1453.173280	56.795365	66.060622
1452.819466	44.517192	66.065626
1452.414779	52.262492	66.070631
1452.247069	48.261770	66.075636
1451.084780	50.956862	66.080641
1450.192289	52.964134	66.085646
1449.715000	46.686705	66.090650
1449.419334	54.230187	66.095655
1448.365109	47.032082	66.100660
1447.240765	50.580547	66.105665
1446.894846	52.409502	66.110670
1446.774052	41.832029	66.115674
1445.734669	51.866906	66.120679
1444.897444	44.609090	66.125684
1444.397330	53.098076	66.130689
1443.926761	45.351502	66.135694
1443.174808	38.521665	66.140698
1441.951289	51.624459	66.145703
1441.807860	43.102109	66.150708
1441.175723	55.677284	66.155713
1440.623082	47.650452	66.160718
1439.815458	48.920450	66.165722
1438.834650	61.443812	66.170727
1438.466791	49.417018	66.175732
1438.144850	41.615291	66.180737
1437.120150	45.004426	66.185742
1436.193394	48.212425	66.190746
1435.434096	48.235315	66.195751
1435.452980	47.421785	66.200756
1434.584373	49.980329	66.205761
1433.702192	57.609137	66.210766
1432.862180	50.343881	66.215770
1432.451228	47.204951	66.220775
1432.252545	52.963756	66.225780
1431.348036	53.519058	66.230785
1430.525407	54.662139	66.235790
1430.007897	48.041039	66.240794
1429.438587	49.216400	66.245799
1428.170819	43.972887	66.250804
1427.643184	52.705935	66.255809
1426.933048	37.218677	66.260814
1426.661801	46.901257	66.265818
1426.159776	52.183168	66.270823
1425.121061	52.136931	66.275828
1424.246415	50.301664	66.280833
1423.828804	49.849226	66.285838
1423.861922	43.590033	66.290842
1422.596581	58.309483	66.295847
1422.016334	60.601442	66.300852
1421.587407	47.542039	66.305857
1420.901163	54.187272	66.310862
1420.104167	32.709053	66.315866
1419.256714	59.784771	66.320871
1418.751989	38.195443	66.325876
1417.628311	56.598053	66.330881
1416.596461	49.347523	66.335886
1416.498472	50.142065	66.340890
1415.775694	55.137378	66.345895
1415.783553	51.184448	66.350900
1415.054485	56.414139	66.355905
1413.884049	45.883643	66.360910
1413.666589	57.191333	66.365914
1412.915379	53.206081	66.370919
1411.460480	54.580536	66.375924
1411.020779	50.455896	66.380929
1410.388658	52.055964	66.385934
1410.439485	53.061811	66.390938
1409.786323	53.685978	66.395943
1408.710084	63.559582	66.400948
1408.069528	45.716437	66.405953
1407.609536	58.713670	66.410958
1407.187686	48.641342	66.415962
1405.607233	61.783539	66.420967
1405.254733	43.981345	66.425972
1404.707231	55.667902	66.430977
1404.156058	51.218796	66.435982
1403.569575	53.775087	66.440986
1402.346085	41.941065	66.445991
1402.200554	47.207318	66.450996
1401.414197	48.212186	66.456001
1400.940959	48.452960	66.461006
1400.369251	54.682619	66.466010
1399.547329	56.273434	66.471015
1399.261137	57.061620	66.476020
1398.105162	52.101539	66.481025
1397.341426	57.923346	66.486030
1397.050762	45.655650	66.491034
1396.471751	52.435224	66.496039
1395.710428	48.415319	66.501044
1394.755301	49.775003	66.506049
1394.136920	49.887467	66.511054
1393.639561	53.236960	66.516058
1392.636267	55.684466	66.521063
1391.854018	61.086613	66.526068
1391.436515	52.560519	66.531073
1390.805863	63.229018	66.536078
1390.651449	50.356217	66.541082
1389.155513	52.270193	66.546087
1389.161295	50.842183	66.551092
1388.516058	53.868266	66.556097
1387.828774	52.417953	66.561102
1386.731350	57.453896	66.566106
1385.632898	61.581720	66.571111
1385.426410	53.230237	66.576116
1385.702933	53.820183	66.581121
1384.298262	58.868693	66.586126
1383.564256	47.655438	66.591130
1382.804015	53.881951	66.596135
1382.300888	52.394485	66.601140
1381.851049	51.994483	66.606145
1380.707687	46.122546	66.611150
1380.291451	54.943545	66.616154
1379.286575	55.596815	66.621159
1379.197229	52.633849	66.626164
1378.678570	61.682434	66.631169
1377.492356	60.650454	66.636174
1377.192941	57.987370	66.641178
1376.516148	54.983739	66.646183
1375.712161	51.308073	66.651188
1374.764160	50.137313	66.656193
1374.314960	61.202729	66.661198
1374.096933	47.427030	66.666202
1373.158253	54.464040	66.671207
1372.458095	54.039174	66.676212
1371.576704	52.391070	66.681217
1371.406467	51.129804	66.686222
1370.492757	44.533850	66.691226
1369.400906	48.151293	66.696231
1368.952448	43.864061	66.701236
1368.808364	44.509819	66.706241
1367.562341	44.971197	66.711246
1367.038497	47.066551	66.716250
1366.010027	52.622949	66.721255
1365.620804	46.615383	66.726260
1365.251989	51.833554	66.731265
1364.729964	54.284995	66.736270
1364.194076	53.570682	66.741274
1363.119328	56.761230	66.746279
1362.576269	42.130494	66.751284
1361.639626	56.736218	66.756289
1360.827630	54.790094	66.761294
1360.747025	44.799153	66.766298
1359.915241	53.631013	66.771303
1359.296519	50.157708	66.776308
1358.282603	46.144851	66.781313
1357.543510	50.288099	66.786318
1357.435731	38.708831	66.791322
1356.652431	50.341408	66.796327
1356.115642	49.180983	66.801332
1355.514065	47.646097	66.806337
1354.758934	48.841548	66.811342
1354.121173	42.021975	66.816346
1353.234243	48.323820	66.821351
1352.766854	51.726899	66.826356
1352.357715	38.766878	66.831361
1351.021880	50.965079	66.836366
1350.500147	40.039787	66.841370
1349.542872	53.182290	66.846375
1349.389628	49.144589	66.851380
1348.904834	54.770686	66.856385
1347.945415	51.964946	66.861390
1347.485996	45.799816	66.866394
1346.939818	57.060410	66.871399
1346.077166	48.335442	66.876404
1345.140269	43.662250	66.881409
1344.569130	58.052193	66.886414
1344.143202	40.819912	66.891418
1343.075071	52.193430	66.896423
1342.307741	42.849369	66.901428
1342.000344	53.635209	66.906433
1341.266807	47.631919	66.911438
1341.041910	42.489177	66.916442
1339.805037	53.634066	66.921447
1339.058572	46.787622	66.926452
1338.647208	42.218546	66.931457
1338.496489	46.148428	66.936462
1337.956989	49.823157	66.941466
1336.524960	60.496048	66.946471
1336.024817	47.925788	66.951476
1335.680587	51.954238	66.956481
1334.433312	49.189530	66.961486
1334.141099	44.431211	66.966490
1333.280339	56.509753	66.971495
1332.902133	53.159064	66.976500
1332.597313	43.340958	66.981505
1331.165482	52.558353	66.986510
1330.695589	43.138632	66.991514
1329.945944	54.816328	66.996519
1329.952884	44.196491	67.001524
1328.853901	52.906836	67.006529
1327.968680	55.624166	67.011534
1327.884137	43.576025	67.016538
1326.583137	61.595284	67.021543
1326.045118	42.647831	67.026548
1325.414254	47.267445	67.031553
1324.641750	45.912695	67.036558
1324.571389	45.220579	67.041562
1323.045702	54.257365	67.046567
1322.555327	51.749219	67.051572
1322.534663	47.013964	67.056577
1321.973269	53.593639	67.061582
1321.107911	47.349548	67.066586
1320.429044	54.100855	67.071591
1320.025526	48.261144	67.076596
1318.791262	46.443659	67.081601
1317.726261	53.368307	67.086606
1317.386334	50.325336	67.091610
1316.777319	60.935212	67.096615
1316.331676	50.164977	67.101620
1315.695807	49.423993	67.106625
1314.447036	59.112171	67.111630
1314.400774	51.654553	67.116634
1313.640838	56.751986	67.121639
1313.228682	49.781447	67.126644
1312.145814	52.244786	67.131649
1311.136179	53.423940	67.136654
1311.090692	52.847713	67.141658
1310.618305	56.603239	67.146663
1309.884861	48.236198	67.151668
1309.490718	50.542746	67.156673
1308.638807	59.357321	67.161678
1307.907027	47.244921	67.166682
1306.676166	42.913354	67.171687
1306.228951	57.498054	67.176692
1305.939968	35.546491	67.181697
1304.900320	52.530763	67.186702
1304.308682	48.665255	67.191706
1303.397452	44.563562	67.196711
1303.210028	44.071399	67.201716
1302.685347	42.845986	67.206721
1301.602666	51.347176	67.211726
1301.032440	41.698997	67.216730
1300.171699	47.864235	67.221735
1299.983193	46.539650	67.226740
1299.110443	46.747765	67.231745
1298.083494	63.154471	67.236750
1297.675516	46.206339	67.241754
1297.177191	52.162585	67.246759
1296.930242	48.947149	67.251764
1295.917241	56.634634	67.256769
1295.138708	49.796457	67.261774
1294.675746	51.746534	67.266778
1293.671857	53.085622	67.271783
1292.976970	45.904582	67.276788
1292.786150	51.818250	67.281793
1292.233398	51.680619	67.286798
1291.146738	40.935037	67.291802
1290.050053	49.108888	67.296807
1289.829141	42.391793	67.301812
1289.332883	57.648156	67.306817
1288.147640	53.829714	67.311822
1287.683518	42.704479	67.316826
1287.138906	51.326705	67.321831
1286.951545	52.630600	67.326836
1286.406261	50.504912	67.331841
1285.008828	55.405669	67.336846
1284.724063	48.195699	67.341850
1283.939212	50.408252	67.346855
1283.084836	52.045259	67.351860
1282.450933	49.176758	67.356865
1281.766866	51.086298	67.361870
1281.625549	51.394168	67.366874
1280.759135	48.373407	67.371879
1279.419875	55.034178	67.376884
1278.867819	44.012807	67.381889
1278.375366	45.510278	67.386894
1278.234064	40.226530	67.391898
1277.729360	48.520727	67.396903
1276.878938	49.179441	67.401908
1276.269294	51.099226	67.406913
1275.232609	53.400703	67.411918
1274.156540	45.394063	67.416922
1273.554719	50.964661	67.421927
1273.069291	37.510614	67.426932
1272.796018	40.179554	67.431937
1272.579323	45.698382	67.436942
1271.758458	44.359222	67.441946
1271.047495	56.131700	67.446951
1270.023370	49.990136	67.451956
1268.951070	41.910366	67.456961
1268.170158	56.871378	67.461966
1267.922406	44.423436	67.466970
1267.544302	51.719843	67.471975
1267.299334	47.442856	67.476980
1266.390512	49.973154	67.481985
1265.460465	54.943109	67.486990
1265.243799	44.951737	67.491994
1263.992673	52.703895	67.496999
1263.409908	42.474276	67.502004
1262.775522	44.811139	67.507009
1262.132489	47.868436	67.512014
1261.307113	47.266399	67.517018
1260.519246	44.340386	67.522023
1260.151071	45.294578	67.527028
1259.728757	47.146738	67.532033
1259.042733	42.902030	67.537038
1258.338026	32.286550	67.542042
1257.359382	52.135783	67.547047
1257.085861	53.369804	67.552052
1256.128486	41.006306	67.557057
1254.992477	47.250011	67.562062
1254.825892	40.055953	67.567066
1254.638102	51.984936	67.572071
1253.424552	46.918970	67.577076
1252.415730	39.467754	67.582081
1251.875640	50.117130	67.587086
1251.688049	49.364812	67.592090
1251.249657	47.748816	67.597095
1250.436503	52.878377	67.602100
1249.971936	45.719078	67.607105
1248.867431	43.942497	67.612110
1247.931931	32.581582	67.617114
1247.335491	46.272253	67.622119
1246.757926	42.516484	67.627124
1246.834820	34.277669	67.632129
1245.764608	48.698074	67.637134
1245.027338	37.363984	67.642138
1244.362799	37.833889	67.647143
1243.828542	41.550375	67.652148
1242.868838	35.333936	67.657153
1241.830021	48.057359	67.662158
1241.230483	42.330831	67.667162
1241.044720	42.546427	67.672167
1240.630958	38.960150	67.677172
1239.520700	46.631573	67.682177
1238.519250	47.361619	67.687182
1238.527987	42.068210	67.692186
1237.852723	52.023179	67.697191
1237.314286	42.295853	67.702196
1236.798310	43.123744	67.707201
1235.809870	45.844898	67.712206
1234.914348	47.734456	67.717210
1234.043605	48.623486	67.722215
1233.443646	48.540679	67.727220
1233.093566	44.479097	67.732225
1232.660811	36.269278	67.737230
1231.834272	47.604412	67.742234
1230.836450	54.687135	67.747239
1230.309936	45.512976	67.752244
1230.102134	38.894728	67.757249
1229.225764	48.974707	67.762254
1228.218570	51.090171	67.767258
1227.548608	43.799541	67.772263
1227.359270	37.695575	67.777268
1226.213576	40.397582	67.782273
1225.320993	44.740299	67.787278
1225.292291	36.111439	67.792282
1224.896636	47.885819	67.797287
1224.212101	45.982552	67.802292
1223.453729	51.939156	67.807297
1222.452059	39.557489	67.812302
1221.800136	40.271388	67.817306
1220.699946	40.346966	67.822311
1220.219687	52.784477	67.827316
1219.813893	47.746204	67.832321
1219.542331	44.268201	67.837326
1218.810869	42.304591	67.842330
1217.804111	41.398688	67.847335
1217.094250	47.585687	67.852340
1217.159206	30.787897	67.857345
1215.724606	46.628669	67.862350
1215.042100	41.102991	67.867354
1214.617397	45.544772	67.872359
1213.866765	42.950306	67.877364
1213.006063	48.637767	67.882369
1212.202155	49.388450	67.887374
1211.976384	35.368039	67.892378
1211.545088	39.908634	67.897383
1210.770403	44.683595	67.902388
1210.039269	40.438193	67.907393
1208.937290	53.892306	67.912398
1208.612781	43.995361	67.917402
1208.250022	45.620449	67.922407
1207.579206	51.536327	67.927412
1206.997077	35.137879	67.932417
1205.574068	58.958984	67.937422
1204.997478	49.658758	67.942426
1204.442293	50.645848	67.947431
1204.014996	39.257754	67.952436
1203.947735	47.581744	67.957441
1202.662823	52.888829	67.962446
1202.100874	59.186351	67.967450
1201.592500	46.839786	67.972455
1200.992944	51.932242	67.977460
1199.861906	54.428514	67.982465
1199.048935	56.645564	67.987470
1198.748473	45.634673	67.992474
1198.342255	45.669294	67.997479
1197.244041	47.370331	68.002484
1197.001537	42.646706	68.007489
1196.006990	38.339121	68.012494
1195.588598	41.355979	68.017498
1194.561574	42.938468	68.022503
1193.969043	48.576984	68.027508
1193.732477	44.150446	68.032513
1192.320800	58.437523	68.037518
1191.743905	41.636137	68.042522
1191.188904	50.474480	68.047527
1190.908679	42.874319	68.052532
1190.552279	46.696568	68.057537
1189.583080	44.289822	68.062542
1188.961925	42.572020	68.067546
1187.963653	47.090819	68.072551
1187.563764	41.917582	68.077556
1186.765168	40.415645	68.082561
1185.949024	50.033495	68.087566
1185.568285	46.804657	68.092570
1185.194358	46.253855	68.097575
1184.406461	38.466356	68.102580
1183.516402	40.632591	68.107585
1182.658897	41.763949	68.112590
1182.504112	45.300260	68.117594
1181.048856	53.988464	68.122599
1180.969354	40.641777	68.127604
1180.569018	43.605306	68.132609
1179.436760	50.061323	68.137614
1178.550434	47.239299	68.142618
1177.784124	47.033155	68.147623
1177.393571	48.186450	68.152628
1177.458937	52.406811	68.157633
1176.587662	45.368974	68.162638
1176.051794	38.925900	68.167642
1175.211407	51.947357	68.172647
1174.349378	51.348024	68.177652
1173.659999	42.311742	68.182657
1172.812160	46.221602	68.187662
1172.435968	37.395705	68.192666
1171.117760	52.748083	68.197671
1170.470898	48.637516	68.202676
1170.295424	37.121083	68.207681
1169.665654	53.538759	68.212686
1169.601036	46.740060	68.217690
1168.638016	46.336553	68.222695
1167.452302	48.526157	68.227700
1167.116354	44.351958	68.232705
1166.376019	45.735911	68.237710
1165.591616	37.769678	68.242714
1164.861202	42.701606	68.247719
1164.496489	56.126795	68.252724
1164.015548	47.609275	68.257729
1162.952054	44.154719	68.262734
1162.353757	50.070111	68.267738
1162.027313	41.417644	68.272743
1161.167704	47.797194	68.277748
1160.374031	41.544925	68.282753
1159.346402	39.492821	68.287758
1159.153256	26.925855	68.292762
1158.529482	46.092642	68.297767
1157.670606	38.398440	68.302772
1157.087861	28.831152	68.307777
1156.286406	35.642976	68.312782
1155.965416	34.839344	68.317786
1155.075430	42.125698	68.322791
1154.288118	42.378619	68.327796
1153.747818	43.402774	68.332801
1153.100810	40.875423	68.337806
1152.478318	30.912353	68.342810
1151.737335	47.011834	68.347815
1151.166017	39.972037	68.352820
1151.121426	36.260840	68.357825
1149.686662	37.301092	68.362830
1149.237216	39.931829	68.367834
1148.919035	43.561931	68.372839
1147.904050	33.002144	68.377844
1147.006674	31.142211	68.382849
1146.303375	37.219372	68.387854
1146.342080	35.401374	68.392858
1144.980454	48.844756	68.397863
1143.979941	38.680039	68.402868
1143.531475	43.567133	68.407873
1143.220554	40.547965	68.412878
1142.945219	40.542858	68.417882
1142.229939	40.052656	68.422887
1141.296898	36.596288	68.427892
1140.768834	37.102860	68.432897
1140.135696	43.974652	68.437902
1139.101649	33.931963	68.442906
1138.656531	43.672153	68.447911
1138.239278	40.275676	68.452916
1137.615250	35.218519	68.457921
1136.356561	49.996918	68.462926
1136.181307	35.123285	68.467930
1135.614607	39.128785	68.472935
1134.254314	45.144866	68.477940
1133.633361	39.786036	68.482945
1132.642347	49.387554	68.487950
1132.675872	41.799005	68.492954
1132.307933	47.245702	68.497959
1131.607420	37.459038	68.502964
1130.682288	40.690529	68.507969
1130.102183	49.573871	68.512974
1129.590627	38.746377	68.517978
1128.207881	47.935556	68.522983
1127.704393	40.363032	68.527988
1127.553734	40.215102	68.532993
1126.981893	45.877144	68.537998
1126.385901	40.492270	68.543002
1125.226141	47.220749	68.548007
1124.495093	42.920169	68.553012
1124.644411	46.119549	68.558017
1123.234185	39.479673	68.563022
1122.884775	35.451121	68.568026
1122.268603	43.964900	68.573031
1121.408164	47.028419	68.578036
1120.733005	44.078221	68.583041
1120.019215	58.828317	68.588046
1119.422011	40.478543	68.593050
1119.066509	41.982645	68.598055
1117.866860	54.179778	68.603060
1117.575443	38.402147	68.608065
1117.007586	47.989982	68.613070
1116.312742	41.488634	68.618074
1115.415652	53.120431	68.623079
1114.773540	45.926330	68.628084
1114.607596	44.211838	68.633089
1113.121261	46.015637	68.638094
1112.281301	40.409384	68.643098
1111.591882	47.378438	68.648103
1111.428113	33.714028	68.653108
1111.656789	36.672135	68.658113
1110.668537	39.853751	68.663118
1109.805581	44.984959	68.668122
1109.185929	42.774953	68.673127
1107.974301	33.657767	68.678132
1107.081272	36.745395	68.683137
1106.664218	40.618295	68.688142
1106.538859	39.909705	68.693146
1105.936040	28.301996	68.698151
1104.845003	43.757021	68.703156
1104.210653	37.249211	68.708161
1103.701452	41.562525	68.713166
1103.137743	34.434807	68.718170
1101.874039	40.583765	68.723175
1101.478885	44.087348	68.728180
1101.271922	42.067161	68.733185
1100.264942	51.466234	68.738190
1099.693610	31.166499	68.743194
1098.989848	43.259528	68.748199
1098.496151	37.719628	68.753204
1098.199441	35.595450	68.758209
1096.821708	38.285534	68.763214
1096.542997	41.680715	68.768218
1095.847720	39.086945	68.773223
1094.745893	36.370190	68.778228
1094.309848	31.959629	68.783233
1093.641073	39.333810	68.788238
1093.354493	29.918124	68.793242
1091.956132	44.761323	68.798247
1091.175266	41.984058	68.803252
1091.231492	25.348524	68.808257
1090.597759	48.312439	68.813262
1090.277710	35.182220	68.818266
1089.206958	33.698374	68.823271
1088.685825	38.235926	68.828276
1087.763036	38.975594	68.833281
1086.522875	44.308724	68.838286
1086.320181	41.422154	68.843290
1085.708950	36.511203	68.848295
1085.289965	39.078760	68.853300
1084.300779	34.683643	68.858305
1083.451258	45.071604	68.863310
1083.014750	43.272423	68.868314
1082.732426	44.143601	68.873319
1082.096369	48.418753	68.878324
1081.040267	37.824539	68.883329
1080.369137	56.287703	68.888334
1080.154510	35.002453	68.893338
1079.198657	44.484855	68.898343
1078.234378	35.202193	68.903348
1077.797601	41.877189	68.908353
1077.500680	42.613501	68.913358
1076.419314	39.426744	68.918362
1075.847781	41.851417	68.923367
1075.113048	43.534111	68.928372
1074.784463	43.395563	68.933377
1073.631069	43.612125	68.938382
1072.973836	33.033318	68.943386
1072.040021	40.742960	68.948391
1071.609122	44.726873	68.953396
1071.746644	31.694183	68.958401
1070.478445	43.856498	68.963406
1069.989731	35.871654	68.968410
1069.214535	46.340833	68.973415
1068.871697	39.368793	68.978420
1068.451254	42.986784	68.983425
1067.575150	43.703264	68.988430
1066.794432	34.728862	68.993434
1065.560391	47.155393	68.998439
1065.141598	39.630913	69.003444
1064.729353	45.068893	69.008449
1064.051394	48.021407	69.013454
1063.455370	40.630769	69.018458
1062.614134	43.606099	69.023463
1061.427752	50.053424	69.028468
1061.699115	35.208110	69.033473
1060.494941	50.689035	69.038478
1060.100907	33.503828	69.043482
1059.634497	49.914445	69.048487
1058.695064	43.392100	69.053492
1058.488508	39.618366	69.058497
1057.049403	42.521650	69.063502
1056.764678	42.164826	69.068506
1056.286180	40.419636	69.073511
1055.512867	40.731859	69.078516
1054.910997	30.505359	69.083521
1054.326204	40.170003	69.088526
1053.732872	34.948724	69.093530
1052.625735	30.898798	69.098535
1051.881270	44.425382	69.103540
1051.796014	38.684911	69.108545
1050.471627	47.213591	69.113550
1049.921501	32.826945	69.118554
1049.186679	37.947247	69.123559
1048.960392	41.829232	69.128564
1048.586875	41.223194	69.133569
1047.100251	46.407899	69.138574
1046.678299	35.099425	69.143578
1046.254963	35.783313	69.148583
1045.514341	41.063804	69.153588
1044.842447	38.682362	69.158593
1043.913519	36.805409	69.163598
1043.702363	40.035314	69.168602
1042.993460	36.853976	69.173607
1041.642867	43.168163	69.178612
1041.575992	48.544900	69.183617
1040.950636	33.804388	69.188622
1040.182702	35.374106	69.193626
1039.086400	45.990558	69.198631
1038.560649	47.919126	69.203636
1038.471126	43.712058	69.208641
1037.761919	45.978876	69.213646
1037.305716	40.854052	69.218650
1036.439567	37.920070	69.223655
1036.004304	44.974858	69.228660
1034.879161	28.233958	69.233665
1033.973824	55.638992	69.238670
1033.667696	40.172792	69.243674
1033.073779	37.830986	69.248679
1032.209174	34.452082	69.253684
1031.393298	34.539282	69.258689
1030.724394	37.007837	69.263694
1030.461753	39.752370	69.268698
1029.914930	40.269833	69.273703
1028.663796	42.001573	69.278708
1028.499730	32.036580	69.283713
1027.786854	44.268258	69.288718
1027.031279	38.352163	69.293722
1026.135645	44.332222	69.298727
1025.253950	38.474035	69.303732
1025.107923	38.281222	69.308737
1024.597344	46.980059	69.313742
1023.757637	44.292597	69.318746
1023.051595	34.459550	69.323751
1022.445690	43.550423	69.328756
1021.840607	34.087652	69.333761
1020.613742	44.909374	69.338766
1020.339704	38.366348	69.343770
1019.885624	38.769716	69.348775
1019.221201	48.752952	69.353780
1018.395276	41.925577	69.358785
1017.284151	41.881564	69.363790
1017.381202	33.213800	69.368794
1016.941885	41.555963	69.373799
1015.123656	40.894345	69.378804
1015.124970	31.997397	69.383809
1014.244978	32.941584	69.388814
1013.921916	41.966962	69.393818
1013.138055	35.749459	69.398823
1012.331988	41.548123	69.403828
1012.276185	36.969860	69.408833
1011.443375	47.438754	69.413838
1010.542218	42.157651	69.418842
1010.018477	41.826241	69.423847
1009.176836	50.241874	69.428852
1008.572370	29.425508	69.433857
1007.837977	36.087934	69.438862
1007.202436	36.398752	69.443866
1006.617944	39.733781	69.448871
1005.711119	39.379741	69.453876
1005.229809	37.841580	69.458881
1004.449392	37.609350	69.463886
1004.077320	37.472998	69.468890
1002.953781	41.578147	69.473895
1002.002417	35.183879	69.478900
1002.012057	30.981542	69.483905
1001.492954	50.253107	69.488910
1000.918273	31.340022	69.493914
999.945318	38.518196	69.498919
999.047612	46.051815	69.503924
998.964535	43.243990	69.508929
997.542405	46.723320	69.513934
997.087897	33.054728	69.518938
996.736950	41.737631	69.523943
996.122287	40.165496	69.528948
995.211094	43.445275	69.533953
994.307216	39.361461	69.538958
993.981401	35.937853	69.543962
993.605972	43.402573	69.548967
992.653978	42.390283	69.553972
992.126008	38.680307	69.558977
991.258153	43.093273	69.563982
990.841488	36.402641	69.568986
989.793508	30.651348	69.573991
988.802889	46.787409	69.578996
988.718618	29.727983	69.584001
987.890727	47.795056	69.589006
987.799945	36.894360	69.594010
987.075793	38.097600	69.599015
986.063869	41.423368	69.604020
985.372492	36.247668	69.609025
984.131434	44.964957	69.614030
983.816835	28.911957	69.619034
983.698433	38.229609	69.624039
982.804942	33.975423	69.629044
982.501616	37.931164	69.634049
981.184501	43.254505	69.639054
980.522604	39.805524	69.644058
980.338057	39.949986	69.649063
979.528411	47.136879	69.654068
978.951950	36.010695	69.659073
977.976609	47.039986	69.664078
977.633966	38.270297	69.669082
976.636749	45.996364	69.674087
975.472809	38.727647	69.679092
975.527646	43.298155	69.684097
974.954002	41.525544	69.689102
974.601552	38.975034	69.694106
973.432941	49.317599	69.699111
972.795418	46.695754	69.704116
972.617186	33.579274	69.709121
971.580763	44.522094	69.714126
971.056239	36.333252	69.719130
970.652050	39.880862	69.724135
969.176047	41.383492	69.729140
968.780009	38.770535	69.734145
967.754305	42.786019	69.739150
967.821513	42.204487	69.744154
967.260271	45.792856	69.749159
966.106458	34.427391	69.754164
965.543392	46.969542	69.759169
965.025957	34.873655	69.764174
964.111217	43.843370	69.769178
963.389579	41.428868	69.774183
962.490580	42.633127	69.779188
962.314156	41.011775	69.784193
961.977766	38.897083	69.789198
961.363285	36.668949	69.794202
960.233041	39.726560	69.799207
959.900729	45.035144	69.804212
959.076484	32.503976	69.809217
958.064676	39.057595	69.814222
957.655721	44.941317	69.819226
957.039085	29.942426	69.824231
955.837788	42.453663	69.829236
955.616879	32.857254	69.834241
954.806199	35.036164	69.839246
954.595776	33.037042	69.844250
953.783631	36.208038	69.849255
952.823337	27.801549	69.854260
952.230063	29.963213	69.859265
951.612014	36.916207	69.864270
951.477408	24.481892	69.869274
950.332438	38.851184	69.874279
949.744482	33.591236	69.879284
949.578907	22.972101	69.884289
948.247945	32.457446	69.889294
947.375061	35.027858	69.894298
946.907953	26.495596	69.899303
946.455940	32.788268	69.904308
946.185013	27.323347	69.909313
944.927887	33.118103	69.914318
944.382164	36.815963	69.919322
943.729592	41.756055	69.924327
942.995056	45.453999	69.929332
942.270345	29.947210	69.934337
941.613812	43.992801	69.939342
941.287147	39.577482	69.944346
940.792977	36.861879	69.949351
939.502432	40.230419	69.954356
939.323968	44.834892	69.959361
938.594043	47.144454	69.964366
937.989914	34.335432	69.969370
937.226007	36.860124	69.974375
936.352440	43.661401	69.979380
936.348510	27.885398	69.984385
934.885655	40.923935	69.989390
934.411251	34.862217	69.994394
933.722711	38.146009	69.999399
933.331130	39.439843	70.004404
932.646155	42.273660	70.009409
931.460533	43.717492	70.014414
931.114096	36.552100	70.019418
930.804717	42.437325	70.024423
930.064558	49.819746	70.029428
929.324585	35.299356	70.034433
928.727337	42.403580	70.039438
928.214607	35.750326	70.044442
927.161537	37.827470	70.049447
926.617023	41.036311	70.054452
926.270250	38.724590	70.059457
924.798017	38.334397	70.064462
924.286170	34.691256	70.069466
923.976442	32.479292	70.074471
923.369181	35.020061	70.079476
923.203367	36.552348	70.084481
921.781672	46.749129	70.089486
921.256186	35.988573	70.094490
920.603151	41.796024	70.099495
920.162754	41.741516	70.104500
919.226929	49.751132	70.109505
918.352547	44.989328	70.114510
917.907830	45.312381	70.119514
917.922410	31.764708	70.124519
916.844179	43.048492	70.129524
916.232267	36.004190	70.134529
915.530930	44.607241	70.139534
914.323871	36.131227	70.144538
913.763181	34.274573	70.149543
913.063671	43.836072	70.154548
913.460355	33.274117	70.159553
912.177557	46.919498	70.164558
911.320865	31.484183	70.169562
910.973545	37.473212	70.174567
910.197615	46.707846	70.179572
909.147985	35.753168	70.184577
908.310058	48.747473	70.189582
907.910227	46.590846	70.194586
907.921134	48.492386	70.199591
906.883057	31.179496	70.204596
906.168027	39.598654	70.209601
905.520076	48.932768	70.214606
905.236942	46.645614	70.219610
903.913660	35.266153	70.224615
903.067660	46.951361	70.229620
902.665105	48.945501	70.234625
902.352945	42.463752	70.239630
901.921133	41.844937	70.244634
900.995361	43.461888	70.249639
900.283607	44.494455	70.254644
899.576758	44.277357	70.259649
898.506322	47.677121	70.264654
898.052242	48.695491	70.269658
897.806987	38.454869	70.274663
896.993505	41.693901	70.279668
896.038528	39.433239	70.284673
895.113128	36.839882	70.289678
894.719548	38.860977	70.294682
894.509806	45.236527	70.299687
893.690510	40.021291	70.304692
893.242077	32.507882	70.309697
891.981493	44.902427	70.314702
891.865120	39.524874	70.319706
890.556662	45.414555	70.324711
889.839887	43.019801	70.329716
889.842535	40.136844	70.334721
889.485983	45.373601	70.339726
888.818720	51.968609	70.344730
887.839304	43.588838	70.349735
886.760370	45.181284	70.354740
885.855146	33.114021	70.359745
885.059090	44.647788	70.364750
884.841345	50.818043	70.369754
884.684116	34.473532	70.374759
884.041582	48.106918	70.379764
883.153679	37.000367	70.384769
882.350225	43.706928	70.389774
882.038728	43.704450	70.394778
881.083869	37.719202	70.399783
880.214774	50.023072	70.404788
880.040915	31.710119	70.409793
878.957643	44.910618	70.414798
878.124824	34.388210	70.419802
877.650399	41.630583	70.424807
876.976917	40.444713	70.429812
876.875117	38.947104	70.434817
875.445352	41.106292	70.439822
875.136904	46.389009	70.444826
874.698381	35.072185	70.449831
873.746970	46.173385	70.454836
872.704113	32.798727	70.459841
871.830717	45.525882	70.464846
871.845207	34.581645	70.469850
871.779350	36.683047	70.474855
870.495049	42.081638	70.479860
869.836401	30.825079	70.484865
868.941009	43.558887	70.489870
868.978253	32.722989	70.494874
867.719661	36.263087	70.499879
866.684990	47.609340	70.504884
866.541462	21.654780	70.509889
865.922423	38.107019	70.514894
865.130121	29.306424	70.519898
864.553539	49.367685	70.524903
863.683249	43.881467	70.529908
863.678424	38.735311	70.534913
862.382857	45.264741	70.539918
861.894551	42.746907	70.544922
861.392599	39.911141	70.549927
860.434818	52.159749	70.554932
860.016781	37.047287	70.559937
858.836256	39.756568	70.564942
858.561419	41.102793	70.569946
858.025178	38.367097	70.574951
857.032278	38.406836	70.579956
856.512504	39.136062	70.584961
855.868504	41.605427	70.589966
855.532130	43.571695	70.594970
854.752323	48.043226	70.599975
853.755972	47.172082	70.604980
853.301004	33.708605	70.609985
852.929673	46.660199	70.614990
852.048631	41.524187	70.619994
851.311696	45.285610	70.624999
850.261697	46.701587	70.630004
850.440253	31.691296	70.635009
849.272057	46.721877	70.640014
848.630990	38.624153	70.645018
848.263624	46.822424	70.650023
847.215786	43.764471	70.655028
846.826976	42.473382	70.660033
846.584200	55.789281	70.665038
845.512203	47.367494	70.670042
844.640649	39.044693	70.675047
843.187229	50.391370	70.680052
843.309188	42.088636	70.685057
842.866842	51.541419	70.690062
841.967502	50.766798	70.695066
841.224231	46.922398	70.700071
840.768194	49.961064	70.705076
840.527952	47.105726	70.710081
839.587567	48.035931	70.715086
838.542004	45.337146	70.720090
838.326792	42.842083	70.725095
837.625141	53.763206	70.730100
837.011380	43.891886	70.735105
836.102864	50.903749	70.740110
835.695646	30.630052	70.745114
834.706173	38.072665	70.750119
833.680705	45.732313	70.755124
833.464172	32.902642	70.760129
832.894142	42.002023	70.765134
832.407054	40.270862	70.770138
831.651192	39.531755	70.775143
830.883997	39.917185	70.780148
830.536595	41.401111	70.785153
829.076000	42.857215	70.790158
828.522812	40.048534	70.795162
827.936664	48.904492	70.800167
827.628938	50.787361	70.805172
827.178532	40.424870	70.810177
825.934749	50.514537	70.815182
825.525887	50.063962	70.820186
825.287378	37.214135	70.825191
824.135016	47.101602	70.830196
823.368352	38.104561	70.835201
822.878417	43.208018	70.840206
822.451257	42.098070	70.845210
821.659057	44.644644	70.850215
820.882817	47.709046	70.855220
820.457721	29.899699	70.860225
819.416855	49.941821	70.865230
818.727924	34.328469	70.870234
818.243889	44.098528	70.875239
817.524732	42.191428	70.880244
817.261755	33.101610	70.885249
816.415818	41.800228	70.890254
815.665923	39.563725	70.895258
815.185464	40.228358	70.900263
814.100135	57.325664	70.905268
813.315542	34.839759	70.910273
812.534750	32.527755	70.915278
812.532409	39.672920	70.920282
812.269307	40.664062	70.925287
811.144574	53.300359	70.930292
810.548584	36.440679	70.935297
809.875185	46.747055	70.940302
808.819649	39.756049	70.945306
807.765432	40.653924	70.950311
807.266171	37.751513	70.955316
807.140190	38.403880	70.960321
806.567330	45.784926	70.965326
805.958316	40.047423	70.970330
805.378631	50.368847	70.975335
804.288506	51.395435	70.980340
804.258461	32.616510	70.985345
803.078313	42.899469	70.990350
802.303828	54.578051	70.995354
801.924203	40.799833	71.000359
800.631372	53.954873	71.005364
800.165813	30.889949	71.010369
799.431129	51.419478	71.015374
798.957701	46.456715	71.020378
799.091104	42.975813	71.025383
798.065924	53.076427	71.030388
797.111740	46.969686	71.035393
796.765696	48.995845	71.040398
796.017404	50.668158	71.045402
795.035264	47.438929	71.050407
794.584601	49.978455	71.055412
793.960529	48.622325	71.060417
792.696807	49.881542	71.065422
792.075147	58.462480	71.070426
792.168780	51.040994	71.075431
791.443784	53.252045	71.080436
790.945792	49.751799	71.085441
789.828020	43.469262	71.090446
789.176399	43.151946	71.095450
788.873521	35.353633	71.100455
787.650664	42.658379	71.105460
787.217267	46.231162	71.110465
786.467593	41.436947	71.115470
785.820502	51.562534	71.120474
784.953270	38.511608	71.125479
784.114781	52.277119	71.130484
784.304974	45.430016	71.135489
783.844085	49.939107	71.140494
782.768267	43.129528	71.145498
781.729487	38.228377	71.150503
780.825244	47.967562	71.155508
780.616467	40.800788	71.160513
780.196151	46.804602	71.165518
779.156786	40.350326	71.170522
778.849114	46.020836	71.175527
778.217956	43.169387	71.180532
777.317934	40.378081	71.185537
776.272602	47.935259	71.190542
776.246826	36.278388	71.195546
775.742182	39.241225	71.200551
774.252167	46.675232	71.205556
774.024704	34.511177	71.210561
773.012194	42.980868	71.215566
772.949932	43.408639	71.220570
772.512611	54.230929	71.225575
771.427883	45.014888	71.230580
770.769564	42.639250	71.235585
770.040785	60.630668	71.240590
769.123370	38.609026	71.245594
768.655486	40.219365	71.250599
767.976829	50.165483	71.255604
767.847800	33.277223	71.260609
766.922746	52.473066	71.265614
766.189599	51.197381	71.270618
765.596484	35.223465	71.275623
764.494874	41.797751	71.280628
763.798137	40.910489	71.285633
762.982936	39.334069	71.290638
762.813168	38.515880	71.295642
762.852632	32.918005	71.300647
761.695672	49.340778	71.305652
761.172205	34.007027	71.310657
760.539564	35.996813	71.315662
759.217386	34.974158	71.320666
758.933812	33.820867	71.325671
758.020575	41.374366	71.330676
757.572625	32.585227	71.335681
756.676684	42.330977	71.340686
755.699836	41.390541	71.345690
755.457057	45.078056	71.350695
754.832239	38.956751	71.355700
754.794237	43.363836	71.360705
753.648132	44.676885	71.365710
752.702586	48.173513	71.370714
752.190430	30.564121	71.375719
751.331179	50.178397	71.380724
750.879925	34.088871	71.385729
749.824076	39.380189	71.390734
749.867716	44.726707	71.395738
749.250088	33.920956	71.400743
748.037061	50.321122	71.405748
747.881422	45.399242	71.410753
747.149272	42.768871	71.415758
745.989656	44.908779	71.420762
745.640109	45.035371	71.425767
745.052925	38.726739	71.430772
744.736825	40.007006	71.435777
743.617929	47.115460	71.440782
742.906468	40.320435	71.445786
742.682839	42.174156	71.450791
741.585786	37.189265	71.455796
740.993098	35.544318	71.460801
740.290345	45.191514	71.465806
739.592823	38.280738	71.470810
738.846557	36.130411	71.475815
738.007863	49.402400	71.480820
737.726463	32.681899	71.485825
737.336192	29.147177	71.490830
736.554932	39.317774	71.495834
735.726294	27.503312	71.500839
734.738678	40.641314	71.505844
734.347621	35.843644	71.510849
733.700377	36.705144	71.515854
733.049629	31.775361	71.520858
732.237543	41.802642	71.525863
731.573881	40.410256	71.530868
731.558500	38.932012	71.535873
730.512258	38.532461	71.540878
729.485165	36.277041	71.545882
729.063503	37.157821	71.550887
728.629797	46.416855	71.555892
727.608882	42.225630	71.560897
727.233865	47.701871	71.565902
726.445246	39.499953	71.570906
725.996728	32.965837	71.575911
724.791264	45.624468	71.580916
724.205178	35.323032	71.585921
723.622254	42.442354	71.590926
723.629557	38.674038	71.595930
723.170062	36.448101	71.600935
722.007495	50.772966	71.605940
721.596170	34.792205	71.610945
720.403249	35.909306	71.615950
719.490120	43.693023	71.620954
719.307643	37.539154	71.625959
718.504621	37.657523	71.630964
717.848489	39.764593	71.635969
716.798318	44.246087	71.640974
716.688670	40.020175	71.645978
716.244557	42.899272	71.650983
715.307409	40.238474	71.655988
714.484191	37.684111	71.660993
713.891239	42.788215	71.665998
713.258194	46.958889	71.671002
712.671864	42.037775	71.676007
711.490387	53.076306	71.681012
711.234505	42.192472	71.686017
710.941346	35.975806	71.691022
709.654744	47.172987	71.696026
709.090340	49.766902	71.701031
708.118839	49.883713	71.706036
708.298743	46.132069	71.711041
707.933549	45.442762	71.716046
706.870217	45.309279	71.721050
706.385543	35.677643	71.726055
705.091191	43.880006	71.731060
704.072056	37.263284	71.736065
703.362428	45.281099	71.741070
703.175668	41.948934	71.746074
702.923295	41.809339	71.751079
702.379648	43.835430	71.756084
701.734360	34.563664	71.761089
700.793273	40.491130	71.766094
700.295154	45.096040	71.771098
699.686227	41.192455	71.776103
698.312251	33.209895	71.781108
697.845879	32.900955	71.786113
697.426949	32.258050	71.791118
696.929363	33.606639	71.796122
696.275576	31.085230	71.801127
695.632957	36.318661	71.806132
695.210044	34.320283	71.811137
693.592671	46.106267	71.816142
693.376508	36.770912	71.821146
693.136556	35.109239	71.826151
691.989504	42.353072	71.831156
691.238434	35.547029	71.836161
690.384450	40.359976	71.841166
690.243379	41.839452	71.846170
689.941107	38.397954	71.851175
688.717283	46.057692	71.856180
688.294225	36.911387	71.861185
687.642914	35.636890	71.866190
686.722960	39.296612	71.871194
686.128128	27.698824	71.876199
685.229867	39.207897	71.881204
684.743574	30.915291	71.886209
684.692201	38.341050	71.891214
683.487921	41.129881	71.896218
683.043399	32.461636	71.901223
682.336147	33.345319	71.906228
681.728235	36.662062	71.911233
680.871926	37.689319	71.916238
680.338568	39.060952	71.921242
679.844964	43.105357	71.926247
678.421106	40.708136	71.931252
677.985840	32.841045	71.936257
677.481106	37.727692	71.941262
677.337032	38.843390	71.946266
676.809668	24.987828	71.951271
675.727027	47.084976	71.956276
675.116101	31.580691	71.961281
673.706392	52.220859	71.966286
673.328555	37.530967	71.971290
673.037734	27.898442	71.976295
672.188907	42.338932	71.981300
672.412279	40.486803	71.986305
671.125629	41.213594	71.991310
670.227239	39.503803	71.996314
669.818494	37.126302	72.001319
668.719582	38.329378	72.006324
668.213770	46.134985	72.011329
667.600595	36.556935	72.016334
667.350533	45.349939	72.021338
666.279622	33.755420	72.026343
665.489475	32.113548	72.031348
665.133194	40.294291	72.036353
664.612894	47.875138	72.041358
663.718666	42.391237	72.046362
663.315097	34.667327	72.051367
662.180727	46.512034	72.056372
661.977659	38.379327	72.061377
660.839492	49.827270	72.066382
660.019577	39.075833	72.071386
660.013756	40.390280	72.076391
659.387582	38.233472	72.081396
658.556952	40.030890	72.086401
657.413924	39.156375	72.091406
656.903425	36.864461	72.096410
656.718387	34.720987	72.101415
656.100560	37.205152	72.106420
655.067413	36.352563	72.111425
654.435002	39.980704	72.116430
653.828379	36.603441	72.121434
652.677097	37.198307	72.126439
652.082669	40.017774	72.131444
651.689463	33.911662	72.136449
651.233333	33.126463	72.141454
650.828064	34.201754	72.146458
649.929767	36.257518	72.151463
648.996994	31.367936	72.156468
649.022074	37.654059	72.161473
647.914766	43.204331	72.166478
647.385382	38.751961	72.171482
646.704317	43.401778	72.176487
645.918786	31.241464	72.181492
645.046004	37.844008	72.186497
644.337315	31.343456	72.191502
643.921127	36.663839	72.196506
643.446141	37.362323	72.201511
642.280316	35.466481	72.206516
641.642815	19.772500	72.211521
641.555593	34.681465	72.216526
640.824568	47.256695	72.221530
640.517400	29.209453	72.226535
639.640689	40.585804	72.231540
638.646359	37.830069	72.236545
637.440108	35.600062	72.241550
636.634861	36.133528	72.246554
636.417869	34.360978	72.251559
635.852741	42.215454	72.256564
635.891948	34.490429	72.261569
634.874991	46.333794	72.266574
633.841083	43.183837	72.271578
633.566694	34.679315	72.276583
632.528557	42.885063	72.281588
632.026441	39.130061	72.286593
631.213763	44.808458	72.291598
630.657155	45.950427	72.296602
630.524398	29.994726	72.301607
629.290900	42.033411	72.306612
628.963028	33.206264	72.311617
628.348663	35.568464	72.316622
627.263157	36.700041	72.321626
626.585982	31.911687	72.326631
625.850651	43.735436	72.331636
625.381119	44.896655	72.336641
624.679437	42.732956	72.341646
623.543673	44.853350	72.346650
623.393781	36.377887	72.351655
623.005669	42.406548	72.356660
622.383732	39.023847	72.361665
621.496869	45.001050	72.366670
620.858120	52.307468	72.371674
620.537833	38.182408	72.376679
619.490212	48.581520	72.381684
618.858978	37.118850	72.386689
618.375483	36.051024	72.391694
617.366382	48.519161	72.396698
616.584436	41.052622	72.401703
615.728836	50.263737	72.406708
615.663922	46.189972	72.411713
615.247527	33.466291	72.416718
614.380500	35.348362	72.421722
613.368552	36.149704	72.426727
613.041007	44.144536	72.431732
611.997100	30.513166	72.436737
611.049576	39.746799	72.441742
610.413642	36.699051	72.446746
610.345035	33.294470	72.451751
609.779539	43.102747	72.456756
609.147419	35.519319	72.461761
608.442981	35.194693	72.466766
607.581289	46.319519	72.471770
607.256957	33.442415	72.476775
606.255487	45.568734	72.481780
605.527108	35.931784	72.486785
605.018730	47.984313	72.491790
603.992149	32.849007	72.496794
603.525140	37.701274	72.501799
602.409682	36.443946	72.506804
602.223147	36.684940	72.511809
601.937050	36.158086	72.516814
601.562730	34.943575	72.521818
600.775862	36.306712	72.526823
599.679581	33.147783	72.531828
598.773297	39.194310	72.536833
598.398436	37.579362	72.541838
597.491594	32.158999	72.546842
597.429338	25.304802	72.551847
596.239180	41.162073	72.556852
595.481599	35.178652	72.561857
594.959266	35.149864	72.566862
594.751339	37.002670	72.571866
593.758042	34.421823	72.576871
592.789422	42.532939	72.581876
592.466496	32.512901	72.586881
591.855807	35.721301	72.591886
590.713875	32.817215	72.596890
590.307737	36.719977	72.601895
589.628930	37.152901	72.606900
589.353719	38.661628	72.611905
588.672630	33.932253	72.616910
587.321855	43.061388	72.621914
587.227609	39.080603	72.626919
586.659719	26.780009	72.631924
586.056547	32.197980	72.636929
584.840773	35.255175	72.641934
584.507185	40.185540	72.646938
583.967322	34.738277	72.651943
582.725677	38.813519	72.656948
582.031416	30.675481	72.661953
581.794764	34.177534	72.666958
581.292688	33.117406	72.671962
581.029269	36.505457	72.676967
580.091891	40.555899	72.681972
579.575224	35.732535	72.686977
578.791533	39.873613	72.691982
577.419478	41.957544	72.696986
577.202527	31.643105	72.701991
576.632111	36.792525	72.706996
575.834779	32.048553	72.712001
574.770578	43.446895	72.717006
574.302684	39.934026	72.722010
574.110047	48.246404	72.727015
573.115964	37.229447	72.732020
572.422979	27.233662	72.737025
571.642176	34.457053	72.742030
571.177657	27.078750	72.747034
570.951333	38.376764	72.752039
569.879984	28.621000	72.757044
569.424986	26.544183	72.762049
569.104177	33.121913	72.767054
567.878264	36.984933	72.772058
566.837064	33.345765	72.777063
566.398259	40.022711	72.782068
565.981579	36.594723	72.787073
565.709006	35.412897	72.792078
564.577383	40.642238	72.797082
564.321094	29.578748	72.802087
563.347564	33.127200	72.807092
563.003518	35.499976	72.812097
562.058789	33.627305	72.817102
561.527860	29.569423	72.822106
560.668082	19.762629	72.827111
559.454530	24.730640	72.832116
559.069096	34.374630	72.837121
558.731320	33.423950	72.842126
558.239657	33.970573	72.847130
557.912749	30.111998	72.852135
556.543246	37.279351	72.857140
556.525237	22.563740	72.862145
555.385330	28.139734	72.867150
554.456002	38.747087	72.872154
554.389036	36.597434	72.877159
553.730141	24.388615	72.882164
552.741029	39.341871	72.887169
551.819027	35.182281	72.892174
551.355247	21.860660	72.897178
551.127274	36.937104	72.902183
549.528926	37.306769	72.907188
549.196581	29.396515	72.912193
548.595241	35.988967	72.917198
547.986059	42.147455	72.922202
547.959182	26.083457	72.927207
546.885671	43.297194	72.932212
546.327591	42.272800	72.937217
545.859578	34.161813	72.942222
544.648636	31.681880	72.947226
543.986798	33.864012	72.952231
543.157474	38.461774	72.957236
543.173327	30.354145	72.962241
542.240249	40.612036	72.967246
541.137063	38.786686	72.972250
540.734487	27.661352	72.977255
540.079800	46.142416	72.982260
539.833620	33.390071	72.987265
538.788060	42.849063	72.992270
538.106979	45.892079	72.997274
537.521836	37.877015	73.002279
537.162833	45.761750	73.007284
536.604828	24.971328	73.012289
535.533362	47.847271	73.017294
535.209482	39.486260	73.022298
534.237640	39.566925	73.027303
533.213950	29.508715	73.032308
532.681575	40.136424	73.037313
532.311241	31.943656	73.042318
531.623677	46.092000	73.047322
530.856409	33.167201	73.052327
530.067926	37.608658	73.057332
529.834949	38.144045	73.062337
529.502860	33.617708	73.067342
528.584375	42.851470	73.072346
527.942123	27.796918	73.077351
527.034247	41.918851	73.082356
525.761083	42.807562	73.087361
525.453880	31.389510	73.092366
524.681942	49.001478	73.097370
524.583917	33.568518	73.102375
523.714660	38.488018	73.107380
523.405036	28.281388	73.112385
522.482819	46.929638	73.117390
522.057942	35.186570	73.122394
521.333813	41.986233	73.127399
519.987826	38.728350	73.132404
520.151281	36.114666	73.137409
518.968260	29.874205	73.142414
517.815724	37.823834	73.147418
517.228868	31.307076	73.152423
517.080618	30.386136	73.157428
516.941151	39.565199	73.162433
515.998881	31.996515	73.167438
515.324049	31.906884	73.172442
515.238172	32.571797	73.177447
513.756687	33.914719	73.182452
512.944572	37.358635	73.187457
512.611664	21.818030	73.192462
511.443369	36.481307	73.197466
510.611216	19.802886	73.202471
510.075629	30.505215	73.207476
509.905150	26.323705	73.212481
509.401964	24.891630	73.217486
508.665755	37.779918	73.222490
508.149879	23.556756	73.227495
507.338409	33.467293	73.232500
506.749420	30.252835	73.237505
505.777278	29.869961	73.242510
504.961332	36.728403	73.247514
504.719910	32.881450	73.252519
504.017998	44.346679	73.257524
503.089554	28.285953	73.262529
502.361776	42.002333	73.267534
501.429218	35.889131	73.272538
501.551345	31.809238	73.277543
500.571294	41.003931	73.282548
499.501276	28.860617	73.287553
499.518601	30.835235	73.292558
498.904351	38.850508	73.297562
498.096028	31.758786	73.302567
497.099429	30.345387	73.307572
496.756311	27.873893	73.312577
496.240934	37.598507	73.317582
495.049351	33.568610	73.322586
494.546201	24.777304	73.327591
494.126581	33.535813	73.332596
493.458337	33.484560	73.337601
492.772206	24.823321	73.342606
491.856783	29.799064	73.347610
491.817791	29.652308	73.352615
490.445462	37.200166	73.357620
489.559714	24.335265	73.362625
489.537678	26.825479	73.367630
488.732125	36.561625	73.372634
488.030474	16.967306	73.377639
486.966179	24.634817	73.382644
486.229707	28.254336	73.387649
486.252786	21.507977	73.392654
485.913680	40.094876	73.397658
485.479127	28.413287	73.402663
484.546889	29.384898	73.407668
483.097035	20.265036	73.412673
482.358775	25.395476	73.417678
481.514684	23.388542	73.422682
481.581668	15.391047	73.427687
480.905105	21.881952	73.432692
480.130977	27.188409	73.437697
479.230665	16.788902	73.442702
478.702502	20.126094	73.447706
478.519738	19.841401	73.452711
477.495858	25.501437	73.457716
476.788534	29.371768	73.462721
476.157232	30.129874	73.467726
475.491119	25.756101	73.472730
474.591197	25.897869	73.477735
473.948892	38.416409	73.482740
473.630555	23.117908	73.487745
473.145955	29.447359	73.492750
471.960810	30.754137	73.497754
471.561816	26.839256	73.502759
471.227773	19.337703	73.507764
470.251234	23.547370	73.512769
469.677793	21.653437	73.517774
468.653429	25.687807	73.522778
468.500856	28.936788	73.527783
467.139093	19.607373	73.532788
466.809357	26.530284	73.537793
466.403333	28.364194	73.542798
465.805292	35.446539	73.547802
464.782517	23.573252	73.552807
464.225370	36.433020	73.557812
463.586643	27.597091	73.562817
463.117616	21.468415	73.567822
462.210457	35.164487	73.572826
461.575102	29.855467	73.577831
460.624248	27.271071	73.582836
460.375832	29.217062	73.587841
459.697310	28.989270	73.592846
458.603101	39.225544	73.597850
458.219787	36.240093	73.602855
457.746193	22.284590	73.607860
457.133604	20.683885	73.612865
456.518173	25.857839	73.617870
455.824757	33.448936	73.622874
455.433417	24.166771	73.627879
454.213326	28.177138	73.632884
453.488317	30.709958	73.637889
452.922108	25.356813	73.642894
452.176795	37.730925	73.647898
451.650289	30.100768	73.652903
450.852799	24.271988	73.657908
450.358550	26.876850	73.662913
449.861086	29.430188	73.667918
448.786109	27.885801	73.672922
448.259632	28.851129	73.677927
447.362318	25.321552	73.682932
447.141528	24.847387	73.687937
446.699409	28.517790	73.692942
445.698798	34.998834	73.697946
444.957677	23.845467	73.702951
444.596487	28.029649	73.707956
444.118515	24.474266	73.712961
443.181411	19.714770	73.717966
442.366780	26.390098	73.722970
442.135920	20.256599	73.727975
440.959786	21.872597	73.732980
440.506152	27.016047	73.737985
439.848131	26.657268	73.742990
439.127875	29.493669	73.747994
438.643255	28.654706	73.752999
437.555285	32.161513	73.758004
437.160690	32.818843	73.763009
436.796252	24.719775	73.768014
435.656848	31.081015	73.773018
435.289834	30.584418	73.778023
434.573340	35.145311	73.783028
434.181065	27.375511	73.788033
433.164927	26.745800	73.793038
432.182797	38.618357	73.798042
432.402919	21.387577	73.803047
431.169776	36.876448	73.808052
430.457587	23.867239	73.813057
429.955881	25.574480	73.818062
429.428076	29.895589	73.823066
428.301729	32.571199	73.828071
427.658585	28.230049	73.833076
427.206608	22.314696	73.838081
426.918269	24.524078	73.843086
425.875990	34.040921	73.848090
425.409584	21.681648	73.853095
424.513319	36.492413	73.858100
424.226936	33.284957	73.863105
423.216288	36.762105	73.868110
422.095422	34.906514	73.873114
422.252060	36.286534	73.878119
421.746879	40.843726	73.883124
420.700048	32.698843	73.888129
419.880778	36.763634	73.893134
419.121198	30.410035	73.898138
418.892381	32.321370	73.903143
417.717943	36.602010	73.908148
416.786304	31.231404	73.913153
416.592334	28.357714	73.918158
416.099726	36.054015	73.923162
415.884064	31.581686	73.928167
414.659749	25.308441	73.933172
414.010102	33.382977	73.938177
413.798946	27.012965	73.943182
412.479145	30.042660	73.948186
412.055477	30.550094	73.953191
411.307220	19.418380	73.958196
410.915741	21.626850	73.963201
410.061596	24.464090	73.968206
409.175656	29.941335	73.973210
408.951645	34.444269	73.978215
408.428163	33.572082	73.983220
407.645189	17.221754	73.988225
406.915451	26.072250	73.993230
406.227154	29.990026	73.998234
405.166064	26.404562	74.003239
404.264677	23.332942	74.008244
403.938923	21.995616	74.013249
403.381285	27.363788	74.018254
403.119229	30.445721	74.023258
402.514915	24.075278	74.028263
401.232000	29.235750	74.033268
400.883439	25.539917	74.038273
400.489995	33.234611	74.043278
399.243152	28.078228	74.048282
398.842403	18.538975	74.053287
398.517479	30.734153	74.058292
397.533511	32.237557	74.063297
396.881711	28.930641	74.068302
396.080005	36.143213	74.073306
395.820434	24.405391	74.078311
394.712077	19.947575	74.083316
393.899200	21.951969	74.088321
393.734450	29.011015	74.093326
392.825420	27.791853	74.098330
392.856229	13.005428	74.103335
391.829452	27.743951	74.108340
391.090701	26.997525	74.113345
390.208204	15.142933	74.118350
389.349348	29.011081	74.123354
388.985402	20.367931	74.128359
388.369179	18.602253	74.133364
387.693853	25.165517	74.138369
386.970861	15.344895	74.143374
386.318733	21.227988	74.148378
386.010937	21.054681	74.153383
384.699809	15.053896	74.158388
383.767950	28.828027	74.163393
383.616233	24.772846	74.168398
383.064913	25.619149	74.173402
382.824289	22.131614	74.178407
381.834270	23.134545	74.183412
381.083019	25.414536	74.188417
380.781278	23.467872	74.193422
379.576801	19.626165	74.198426
378.708721	21.730817	74.203431
378.611187	30.344977	74.208436
377.801679	28.625867	74.213441
376.934522	30.580572	74.218446
375.798232	24.384782	74.223450
375.872939	15.685936	74.228455
375.297854	30.439221	74.233460
374.447217	30.768702	74.238465
373.786158	25.665646	74.243470
373.233778	42.947767	74.248474
372.779238	30.123015	74.253479
371.440827	32.435069	74.258484
370.654344	40.193972	74.263489
370.627408	25.527119	74.268494
369.928605	35.802912	74.273498
369.216445	28.177134	74.278503
368.286040	26.374794	74.283508
367.663585	30.506003	74.288513
367.449627	32.187906	74.293518
366.415728	32.171298	74.298522
365.819780	34.298822	74.303527
365.077373	29.468912	74.308532
364.683863	38.652180	74.313537
363.822520	24.544038	74.318542
363.136948	32.053483	74.323546
362.801729	23.062004	74.328551
361.782715	35.001952	74.333556
361.097707	28.138205	74.338561
360.726525	24.425485	74.343566
359.857639	35.321281	74.348570
359.357692	24.922682	74.353575
358.499584	26.883835	74.358580
358.053648	39.244950	74.363585
357.581882	29.221882	74.368590
356.017423	32.213324	74.373594
355.590182	17.490427	74.378599
355.314612	38.728932	74.383604
354.959559	25.367973	74.388609
354.260924	30.593051	74.393614
353.078075	23.874866	74.398618
353.105858	22.276221	74.403623
352.088092	34.897176	74.408628
351.236307	28.580373	74.413633
350.908855	21.401052	74.418638
350.184122	35.441795	74.423642
349.288736	17.693386	74.428647
348.425375	32.634529	74.433652
347.853845	36.025964	74.438657
347.767589	30.046042	74.443662
346.722684	38.327072	74.448666
345.879899	30.730000	74.453671
345.328634	31.730836	74.458676
344.761603	35.708147	74.463681
343.665830	27.596336	74.468686
342.755250	35.398670	74.473690
342.329496	23.409815	74.478695
342.117091	32.641487	74.483700
341.704556	35.075661	74.488705
341.167058	31.236490	74.493710
340.204415	40.442647	74.498714
339.823265	34.698940	74.503719
338.575310	35.785567	74.508724
338.123726	37.120584	74.513729
337.495706	32.672978	74.518734
336.698039	28.156218	74.523738
335.749500	33.265015	74.528743
335.237530	33.841723	74.533748
334.660907	32.735183	74.538753
334.691125	33.591324	74.543758
333.539989	41.829367	74.548762
332.934203	23.411950	74.553767
331.965393	37.130491	74.558772
331.546832	36.440285	74.563777
330.567749	23.913595	74.568782
329.834373	36.454547	74.573786
329.254808	34.919571	74.578791
329.067087	39.997012	74.583796
328.547302	26.621312	74.588801
327.645816	28.182558	74.593806
326.755063	29.481911	74.598810
326.442093	34.896259	74.603815
325.051324	43.440560	74.608820
324.465577	36.543659	74.613825
324.331062	31.131216	74.618830
323.472948	37.135457	74.623834
323.443438	28.847430	74.628839
322.425066	35.348691	74.633844
321.525755	33.678602	74.638849
321.283467	31.653089	74.643854
319.928774	40.970612	74.648858
319.868712	27.313507	74.653863
319.165703	33.294607	74.658868
317.790461	29.499065	74.663873
317.253691	23.475833	74.668878
316.736675	40.416445	74.673882
316.516242	23.741556	74.678887
315.943412	35.462187	74.683892
315.161938	36.129154	74.688897
314.180769	28.178857	74.693902
313.613409	36.546210	74.698906
313.493802	22.092823	74.703911
312.034130	34.382113	74.708916
311.589802	31.009045	74.713921
311.391214	21.839696	74.718926
310.189908	36.290688	74.723930
309.665784	30.833110	74.728935
309.256939	31.517961	74.733940
308.449392	28.701067	74.738945
307.937286	24.723826	74.743950
306.812456	40.193903	74.748954
306.634785	21.481206	74.753959
306.018511	26.522866	74.758964
304.920155	26.503942	74.763969
304.538587	25.240176	74.768974
303.854187	26.516113	74.773978
302.905389	27.452585	74.778983
302.037254	29.170941	74.783988
301.699154	40.772173	74.788993
301.243382	33.882950	74.793998
300.390221	35.069095	74.799002
299.527298	28.916505	74.804007
299.297452	43.767744	74.809012
298.580431	37.937231	74.814017
298.066238	19.962527	74.819022
296.797127	35.253758	74.824026
296.542766	28.223636	74.829031
296.028548	27.517145	74.834036
295.081063	38.846507	74.839041
294.704424	24.008334	74.844046
293.688801	26.678968	74.849050
293.433594	34.468327	74.854055
292.133047	34.735506	74.859060
291.385515	43.218307	74.864065
291.318246	28.204676	74.869070
290.833457	37.050854	74.874074
290.102892	33.365461	74.879079
289.024909	32.192187	74.884084
288.797471	24.974862	74.889089
288.303180	38.393875	74.894094
286.956980	32.893865	74.899098
286.436502	30.661971	74.904103
285.923692	36.489772	74.909108
285.396850	34.068093	74.914113
284.313730	27.209478	74.919118
283.835028	31.790853	74.924122
283.449903	18.791083	74.929127
283.122727	33.586864	74.934132
281.778707	26.094936	74.939137
281.350514	29.171819	74.944142
280.773994	41.791857	74.949146
279.786839	24.855997	74.954151
279.131397	35.326732	74.959156
278.698700	29.255385	74.964161
278.646566	35.590050	74.969166
277.117838	36.272051	74.974170
276.189254	30.235585	74.979175
275.913997	30.333057	74.984180
275.489329	37.936549	74.989185
274.669064	28.878899	74.994190
273.540914	35.049186	74.999194
273.361924	22.096984	75.004199
273.230111	27.427270	75.009204
271.967860	36.370554	75.014209
271.460642	25.203633	75.019214
270.480334	28.740652	75.024218
270.266056	26.225009	75.029223
269.336157	27.172674	75.034228
268.976716	33.114795	75.039233
268.622691	35.771454	75.044238
267.362543	28.070635	75.049242
266.707436	31.978424	75.054247
266.417523	34.639056	75.059252
265.562811	29.909077	75.064257
264.783511	25.274307	75.069262
263.913390	31.611617	75.074266
263.462038	21.913316	75.079271
262.887602	25.346227	75.084276
261.866563	24.297923	75.089281
261.244077	31.690106	75.094286
260.494056	30.683758	75.099290
260.235268	21.861461	75.104295
259.951399	35.059289	75.109300
258.900401	29.028150	75.114305
258.425670	16.665532	75.119310
257.711873	39.484504	75.124314
256.611482	19.797742	75.129319
255.923937	31.132983	75.134324
255.574070	17.706583	75.139329
255.327287	17.758520	75.144334
254.234739	19.413317	75.149338
253.362616	27.660525	75.154343
252.979215	18.334576	75.159348
251.941745	34.921347	75.164353
251.181029	25.611381	75.169358
250.398166	30.192356	75.174362
250.097604	21.994849	75.179367
249.981384	16.027604	75.184372
249.270398	30.966552	75.189377
248.692588	22.393791	75.194382
247.653134	28.513680	75.199386
247.030259	14.468518	75.204391
245.869271	31.409268	75.209396
245.139173	16.329429	75.214401
244.879171	25.376305	75.219406
244.553952	25.052837	75.224410
243.857848	21.175901	75.229415
243.076470	29.719289	75.234420
242.085559	25.053605	75.239425
242.048917	22.687838	75.244430
241.117110	28.055755	75.249434
240.302823	23.790826	75.254439
239.970795	28.884959	75.259444
239.146408	32.557978	75.264449
238.467971	40.064737	75.269454
237.588766	27.236762	75.274458
237.074440	25.812829	75.279463
236.059710	38.865395	75.284468
235.188494	25.020652	75.289473
234.978572	29.515038	75.294478
234.266965	27.077093	75.299482
233.963622	20.691846	75.304487
233.102979	38.789455	75.309492
232.206703	27.296652	75.314497
231.886093	34.788949	75.319502
231.189032	28.775520	75.324506
230.548379	30.722553	75.329511
229.617844	30.599646	75.334516
228.952632	29.204496	75.339521
228.960518	26.984586	75.344526
227.721938	25.286615	75.349530
227.206400	34.363190	75.354535
226.728106	31.262044	75.359540
225.661160	32.589517	75.364545
225.024782	28.100704	75.369550
224.249508	37.396867	75.374554
223.883764	28.490703	75.379559
223.282858	21.892707	75.384564
222.305839	32.050454	75.389569
221.724132	24.645197	75.394574
221.022718	32.683866	75.399578
220.642283	25.155070	75.404583
219.906709	29.649672	75.409588
219.271858	33.951612	75.414593
218.828533	25.846248	75.419598
217.639814	33.555766	75.424602
216.989783	27.687801	75.429607
216.850912	27.815576	75.434612
216.195521	26.387328	75.439617
215.235390	22.098351	75.444622
214.227048	24.495058	75.449626
213.960896	30.658842	75.454631
213.268270	31.590781	75.459636
212.581373	32.450849	75.464641
211.997591	22.109815	75.469646
211.260679	26.246685	75.474650
211.015164	28.190656	75.479655
210.314598	20.282412	75.484660
209.289064	35.265202	75.489665
208.752912	20.376797	75.494670
207.747979	33.661179	75.499674
206.933473	22.667837	75.504679
206.522437	23.468164	75.509684
206.033219	17.368004	75.514689
205.654460	34.404837	75.519694
204.411061	25.594432	75.524698
203.656253	22.497950	75.529703
203.450350	32.039224	75.534708
203.029824	31.257897	75.539713
202.248644	18.972530	75.544718
201.043573	29.562425	75.549722
200.924399	29.366958	75.554727
200.491124	31.938491	75.559732
199.182359	31.300335	75.564737
198.589846	23.218760	75.569742
198.003849	28.618293	75.574746
197.418184	33.517911	75.579751
196.545300	34.882267	75.584756
195.598032	45.729106	75.589761
195.385901	29.087612	75.594766
194.974453	33.022803	75.599770
194.192399	34.424717	75.604775
193.071018	25.235343	75.609780
192.602767	29.226895	75.614785
192.586249	17.281658	75.619790
191.783734	27.586623	75.624794
190.649553	20.617936	75.629799
190.149516	21.170694	75.634804
189.505008	26.803470	75.639809
188.811626	31.534191	75.644814
187.839108	40.171143	75.649818
187.776910	21.252425	75.654823
187.112478	31.284661	75.659828
186.283823	30.864848	75.664833
185.793369	26.754884	75.669838
185.166751	39.720364	75.674842
184.289822	31.360872	75.679847
183.472558	21.082299	75.684852
182.717322	29.876985	75.689857
182.635455	34.620604	75.694862
181.170870	30.732159	75.699866
180.709870	27.487927	75.704871
180.554846	26.344177	75.709876
179.606116	19.919909	75.714881
178.900191	22.843973	75.719886
177.877145	36.883414	75.724890
177.635925	18.898359	75.729895
176.785996	33.599287	75.734900
175.829075	37.170459	75.739905
175.540208	25.032106	75.744910
175.197050	44.777048	75.749914
174.805926	25.387247	75.754919
173.980302	29.093595	75.759924
173.199625	39.656850	75.764929
172.582486	32.205218	75.769934
171.030107	36.185114	75.774938
170.576705	33.769100	75.779943
170.177390	29.267740	75.784948
169.761938	32.017775	75.789953
169.462111	26.677435	75.794958
168.285625	37.411016	75.799962
167.535775	19.746731	75.804967
167.090903	32.683233	75.809972
166.289062	27.457616	75.814977
165.758295	25.567994	75.819982
164.898265	34.803568	75.824986
164.688843	17.821062	75.829991
163.651300	33.105379	75.834996
162.881958	30.271408	75.840001
162.556380	28.342766	75.845006
161.919346	25.312672	75.850010
161.131057	29.087185	75.855015
160.263097	29.498344	75.860020
159.589807	28.588598	75.865025
159.426536	22.780240	75.870030
157.990062	28.291715	75.875034
157.625637	17.669742	75.880039
157.160834	33.827789	75.885044
156.798738	20.909535	75.890049
155.949975	26.675800	75.895054
155.222543	27.979135	75.900058
154.641164	35.273327	75.905063
153.674498	18.225479	75.910068
152.628169	28.525172	75.915073
152.577614	20.251561	75.920078
151.859207	22.650951	75.925082
151.706981	30.833875	75.930087
150.386612	19.030285	75.935092
149.585468	33.789669	75.940097
149.406479	14.960547	75.945102
148.641710	28.665516	75.950106
147.640424	16.230775	75.955111
146.938879	15.235657	75.960116
146.342244	30.957430	75.965121
146.121377	12.937610	75.970126
145.623780	30.933189	75.975130
144.625464	17.719007	75.980135
144.266074	30.236626	75.985140
143.107453	26.526495	75.990145
142.571316	31.686292	75.995150
141.499551	32.751234	76.000154
141.508418	32.723002	76.005159
140.504460	34.247038	76.010164
139.625889	25.145131	76.015169
139.305175	31.904209	76.020174
138.710572	21.260592	76.025178
138.321759	25.562742	76.030183
137.169704	23.038942	76.035188
136.521817	21.899662	76.040193
136.574821	28.696920	76.045198
135.171147	16.826204	76.050202
134.653402	32.246836	76.055207
134.051360	21.851974	76.060212
133.229501	32.524294	76.065217
132.618843	17.997862	76.070222
131.802932	30.725454	76.075226
131.259270	25.247390	76.080231
130.839408	20.124882	76.085236
130.164730	22.775910	76.090241
129.504004	23.947199	76.095246
128.558577	26.590937	76.100250
128.411047	21.555887	76.105255
127.387104	28.947448	76.110260
126.522014	19.206351	76.115265
126.079510	14.022805	76.120270
125.529756	37.462135	76.125274
124.902147	22.880061	76.130279
123.937319	25.492202	76.135284
123.322534	14.829738	76.140289
123.032483	18.174757	76.145294
122.035100	17.321426	76.150298
121.060593	23.576075	76.155303
120.625437	23.254385	76.160308
120.337498	18.497176	76.165313
119.291905	21.940584	76.170318
118.638285	23.479727	76.175322
118.329531	20.789943	76.180327
117.837159	16.287667	76.185332
116.782789	24.463048	76.190337
116.163679	15.491667	76.195342
115.363958	18.580502	76.200346
114.782367	22.776204	76.205351
113.845642	14.853617	76.210356
113.234242	28.608250	76.215361
112.897901	22.296092	76.220366
112.490539	21.659331	76.225370
111.993295	30.712500	76.230375
110.777204	22.402394	76.235380
110.141970	31.764554	76.240385
110.144920	18.592581	76.245390
108.559994	27.563723	76.250394
107.954339	13.001818	76.255399
107.861318	23.660422	76.260404
106.572267	25.253580	76.265409
105.959810	18.556545	76.270414
105.368712	23.710917	76.275418
105.210752	21.011283	76.280423
104.703971	26.134866	76.285428
103.962477	24.614730	76.290433
103.507090	23.102587	76.295438
102.269991	29.550492	76.300442
101.248842	17.052715	76.305447
100.742152	22.061173	76.310452
100.234354	34.892601	76.315457
100.001910	22.256447	76.320462
98.890707	20.975024	76.325466
98.177147	22.615187	76.330471
97.897762	23.392963	76.335476
97.207059	23.566159	76.340481
96.719693	9.143087	76.345486
95.743637	29.081952	76.350490
95.009724	21.063958	76.355495
94.187568	19.045784	76.360500
93.197884	27.734377	76.365505
92.897768	25.555697	76.370510
92.676047	23.708273	76.375514
92.187655	14.550487	76.380519
91.273203	28.381829	76.385524
90.365778	32.804524	76.390529
90.067104	23.539217	76.395534
88.683509	29.893800	76.400538
88.165367	25.313641	76.405543
87.876821	25.268182	76.410548
87.051632	32.826750	76.415553
86.387607	27.044634	76.420558
85.171392	29.108707	76.425562
85.032227	16.386730	76.430567
84.986760	36.055801	76.435572
84.124505	16.307535	76.440577
83.444565	16.245644	76.445582
82.835319	30.632258	76.450586
81.706542	21.819421	76.455591
80.891383	14.238565	76.460596
80.133334	29.412104	76.465601
80.135798	7.155950	76.470606
79.033863	26.466800	76.475610
78.353124	31.337448	76.480615
77.499262	21.039528	76.485620
77.120527	27.535062	76.490625
76.861025	24.037964	76.495630
75.648577	13.161757	76.500634
75.217135	18.489358	76.505639
74.546171	22.085922	76.510644
74.212160	25.901552	76.515649
73.412666	21.667442	76.520654
72.201108	30.363039	76.525658
72.451583	16.618626	76.530663
71.487446	22.450616	76.535668
69.931674	30.926730	76.540673
69.794071	22.003151	76.545678
68.847686	13.246393	76.550682
68.631232	15.756561	76.555687
68.150267	11.443280	76.560692
67.054776	27.280871	76.565697
66.836399	17.977538	76.570702
66.363010	26.749378	76.575706
65.346637	11.125535	76.580711
64.660195	24.745488	76.585716
64.361412	28.013064	76.590721
63.788481	24.338880	76.595726
62.728781	31.425525	76.600730
62.295853	16.971701	76.605735
61.255517	21.745160	76.610740
60.277247	23.336088	76.615745
59.997006	20.621267	76.620750
59.182537	29.389157	76.625754
58.956275	17.321276	76.630759
57.763526	16.134873	76.635764
56.955220	29.088333	76.640769
56.868595	17.830765	76.645774
56.319968	11.755891	76.650778
55.674282	25.074475	76.655783
54.807059	21.743673	76.660788
54.075874	30.812078	76.665793
53.248575	21.019259	76.670798
52.283011	21.862311	76.675802
51.828964	22.275307	76.680807
51.354571	15.463240	76.685812
50.951242	29.875363	76.690817
50.371744	23.966247	76.695822
49.271864	23.353205	76.700826
48.628438	21.024289	76.705831
48.519389	19.199900	76.710836
47.499131	25.633747	76.715841
46.859463	17.622819	76.720846
46.221379	9.673141	76.725850
45.431537	25.446226	76.730855
44.734219	11.510786	76.735860
43.610005	23.290982	76.740865
43.729794	15.988371	76.745870
43.365596	22.697617	76.750874
42.377588	17.151678	76.755879
41.795215	23.022140	76.760884
40.970017	26.121369	76.765889
40.169254	17.981602	76.770894
39.043203	19.102549	76.775898
38.959068	13.910756	76.780903
38.420957	26.385915	76.785908
37.199804	26.787215	76.790913
36.541248	24.151651	76.795918
35.881941	26.341387	76.800922
35.508718	24.666354	76.805927
35.263038	17.535559	76.810932
34.429620	22.105730	76.815937
33.593154	11.664723	76.820942
33.176891	24.888378	76.825946
32.667996	20.133306	76.830951
31.565187	10.684044	76.835956
30.560932	26.207491	76.840961
30.300978	19.854786	76.845966
29.858556	22.407302	76.850970
28.966675	16.194799	76.855975
28.060014	25.023125	76.860980
27.678393	14.012871	76.865985
27.266533	12.001825	76.870990
26.073380	18.002808	76.875994
25.316501	26.968087	76.880999
25.313624	17.721853	76.886004
24.631368	25.312828	76.891009
24.013690	16.066878	76.896014
23.312502	25.352838	76.901018
22.471484	26.825704	76.906023
21.631777	22.639025	76.911028
20.937162	24.440181	76.916033
20.556027	21.317282	76.921038
19.724757	32.591909	76.926042
18.862279	26.116112	76.931047
18.355374	28.250010	76.936052
17.740398	18.636222	76.941057
17.457609	16.240339	76.946062
16.279890	34.580920	76.951066
15.420285	27.467615	76.956071
15.261837	12.175302	76.961076
14.482990	20.158549	76.966081
13.770522	14.705867	76.971086
13.184281	27.855715	76.976090
12.413739	26.955214	76.981095
12.043473	18.447198	76.986100
10.855581	30.185530	76.991105
10.332776	23.322848	76.996110
9.913874	32.065508	77.001114
9.374718	30.349138	77.006119
8.552605	22.947601	77.011124
7.806855	33.612541	77.016129
7.630985	23.870378	77.021134
6.585740	24.467552	77.026139
5.370729	13.560260	77.031143
5.440265	16.083164	77.036148
4.646764	30.404560	77.041153
4.241314	21.246184	77.046158