Mon Mar 08 19:07:35 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.205112	108.670822	0.000000
-1.769370	95.261298	0.005005
-2.548367	61.287493	0.010010
-3.901942	-4.950076	0.015014
-7.580520	-17.444882	0.020019
-13.051665	-27.034596	0.025024
-18.148515	-20.775148	0.030029
-23.107710	-24.087058	0.035034
-27.045149	-29.881486	0.040038
-30.918075	-17.956088	0.045043
-34.235078	-20.344135	0.050048
-37.873261	-27.741057	0.055053
-42.018536	-23.309545	0.060058
-45.404301	-27.771203	0.065062
-49.360584	-27.286724	0.070067
-52.968583	-27.047019	0.075072
-56.838631	-28.124751	0.080077
-60.830804	-19.327680	0.085082
-64.429415	-35.282128	0.090086
-68.386638	-19.008470	0.095091
-72.074725	-22.904654	0.100096
-75.483602	-27.939709	0.105101
-79.168929	-21.000208	0.110106
-83.024006	-28.865472	0.115110
-86.955632	-32.129881	0.120115
-90.771215	-32.058840	0.125120
-94.340541	-31.055741	0.130125
-98.377736	-29.523861	0.135130
-102.041578	-21.056635	0.140134
-106.099413	-28.337613	0.145139
-109.617065	-24.092850	0.150144
-113.212050	-33.678901	0.155149
-117.202938	-25.429118	0.160154
-120.696577	-33.825036	0.165158
-124.548183	-27.917009	0.170163
-127.758954	-33.218543	0.175168
-131.975338	-19.636121	0.180173
-135.866433	-37.943744	0.185178
-139.298910	-40.212298	0.190182
-143.475964	-39.088507	0.195187
-147.200795	-40.436827	0.200192
-151.251093	-28.807791	0.205197
-155.220848	-27.523104	0.210202
-158.877326	-22.879253	0.215206
-162.648122	-24.972374	0.220211
-166.303734	-24.997698	0.225216
-169.694987	-19.896292	0.230221
-173.709345	-16.327487	0.235226
-177.048028	-28.105161	0.240230
-180.914866	-23.528628	0.245235
-184.732578	-24.609775	0.250240
-188.611879	-26.524701	0.255245
-192.408009	-19.540548	0.260250
-195.883976	-30.805883	0.265254
-199.937715	-15.330281	0.270259
-203.357716	-27.798213	0.275264
-207.143781	-23.160418	0.280269
-211.283629	-22.424045	0.285274
-215.057423	-27.452694	0.290278
-218.951590	-20.156409	0.295283
-222.440126	-19.864559	0.300288
-226.434008	-24.019184	0.305293
-230.004335	-26.847465	0.310298
-233.647832	-23.971645	0.315302
-237.673828	-19.347546	0.320307
-241.289960	-30.667706	0.325312
-244.858135	-23.888580	0.330317
-249.068534	-14.819858	0.335322
-252.328008	-31.009462	0.340326
-256.328205	-25.414962	0.345331
-259.864572	-29.470673	0.350336
-263.593035	-37.365297	0.355341
-267.805036	-20.044658	0.360346
-271.230615	-26.221550	0.365350
-275.140087	-26.218805	0.370355
-278.959988	-31.995298	0.375360
-282.371020	-29.162820	0.380365
-286.322185	-20.554859	0.385370
-290.150020	-32.167553	0.390374
-294.255167	-21.215461	0.395379
-297.946843	-24.588781	0.400384
-301.516666	-23.949551	0.405389
-304.993776	-16.773317	0.410394
-308.705226	-26.431927	0.415398
-312.615219	-16.569018	0.420403
-316.341049	-26.132286	0.425408
-320.207344	-31.954918	0.430413
-324.245167	-16.323986	0.435418
-328.121594	-28.460258	0.440422
-331.540360	-24.167894	0.445427
-334.761238	-34.480317	0.450432
-338.871182	-26.338906	0.455437
-342.733795	-23.252914	0.460442
-346.619320	-40.331100	0.465446
-350.791103	-28.450563	0.470451
-354.226595	-27.261882	0.475456
-357.831090	-19.428196	0.480461
-361.474527	-29.505977	0.485466
-365.454644	-30.841585	0.490470
-369.429707	-28.637977	0.495475
-372.837207	-29.962498	0.500480
-376.801739	-29.912952	0.505485
-380.434555	-24.685968	0.510490
-383.858553	-32.368828	0.515494
-387.894302	-26.634409	0.520499
-391.860136	-31.244204	0.525504
-395.425492	-29.744590	0.530509
-399.420071	-25.913669	0.535514
-402.967484	-24.377488	0.540518
-406.711089	-22.587641	0.545523
-410.320694	-37.792327	0.550528
-414.345422	-23.036927	0.555533
-418.500689	-21.838875	0.560538
-421.865504	-30.835178	0.565542
-425.825938	-29.802255	0.570547
-429.416041	-26.051639	0.575552
-433.047267	-28.308531	0.580557
-436.822738	-24.581916	0.585562
-440.372655	-27.460442	0.590566
-444.397221	-22.522444	0.595571
-448.133846	-38.026883	0.600576
-451.875388	-30.024538	0.605581
-456.008492	-17.774711	0.610586
-459.276987	-30.638569	0.615590
-463.588570	-25.069698	0.620595
-467.071408	-31.893117	0.625600
-470.671888	-32.664744	0.630605
-474.576966	-27.655900	0.635610
-478.282163	-24.661061	0.640614
-482.052664	-21.551716	0.645619
-485.696564	-29.219803	0.650624
-489.092669	-18.670774	0.655629
-493.461289	-27.806260	0.660634
-496.884787	-30.428942	0.665638
-500.801893	-24.311192	0.670643
-504.690394	-33.245807	0.675648
-508.592961	-19.466914	0.680653
-512.185699	-20.416322	0.685658
-515.670323	-32.294738	0.690662
-519.935678	-14.463741	0.695667
-523.425127	-32.148886	0.700672
-526.974888	-30.385083	0.705677
-531.061351	-37.474664	0.710682
-534.445780	-33.012477	0.715686
-538.473847	-20.716224	0.720691
-542.331558	-35.467930	0.725696
-545.813564	-25.625727	0.730701
-549.886243	-28.253442	0.735706
-553.219478	-22.425975	0.740710
-557.294194	-33.820587	0.745715
-561.385008	-29.176149	0.750720
-564.471929	-27.246542	0.755725
-568.509354	-17.653028	0.760730
-572.383093	-36.044623	0.765734
-576.106788	-19.028566	0.770739
-580.227881	-27.427618	0.775744
-583.576017	-32.011186	0.780749
-587.421943	-25.903093	0.785754
-590.528000	-33.097148	0.790758
-594.763343	-17.869462	0.795763
-598.401224	-40.748527	0.800768
-602.611719	-27.363402	0.805773
-606.522370	-32.199248	0.810778
-610.022084	-30.714535	0.815782
-613.708505	-25.775092	0.820787
-617.352412	-31.372573	0.825792
-621.130574	-36.046645	0.830797
-624.955165	-20.255375	0.835802
-628.691727	-38.787042	0.840806
-632.691440	-30.749491	0.845811
-636.196986	-31.540764	0.850816
-639.872808	-31.741895	0.855821
-643.829093	-29.162395	0.860826
-647.385562	-37.768213	0.865830
-651.381555	-23.488518	0.870835
-655.075628	-25.881671	0.875840
-658.390829	-34.652168	0.880845
-662.862977	-33.086119	0.885850
-666.340937	-41.456884	0.890854
-670.163312	-19.636075	0.895859
-673.889655	-39.419727	0.900864
-677.497583	-32.228393	0.905869
-681.750006	-24.554052	0.910874
-685.354643	-35.432223	0.915878
-689.256452	-38.807610	0.920883
-692.655402	-35.235375	0.925888
-695.869568	-29.661695	0.930893
-699.949511	-26.174583	0.935898
-703.665469	-33.517010	0.940902
-707.805315	-29.165668	0.945907
-711.542165	-33.779966	0.950912
-714.938163	-36.212769	0.955917
-719.044827	-29.123013	0.960922
-722.688247	-35.734308	0.965926
-726.826848	-31.102456	0.970931
-730.456274	-34.180705	0.975936
-733.997439	-33.001400	0.980941
-738.048640	-21.189959	0.985946
-741.871755	-36.440385	0.990950
-745.458468	-30.403434	0.995955
-749.058488	-27.220001	1.000960
-752.519057	-24.191303	1.005965
-756.457988	-23.050891	1.010970
-760.197910	-25.703035	1.015974
-764.181440	-24.911847	1.020979
-768.107074	-26.294904	1.025984
-772.026604	-26.985121	1.030989
-775.457848	-28.414065	1.035994
-778.897655	-35.016814	1.040998
-782.936695	-21.158936	1.046003
-786.880963	-38.531261	1.051008
-790.749800	-32.239433	1.056013
-794.678108	-31.972646	1.061018
-797.847516	-31.760923	1.066022
-801.774306	-31.018162	1.071027
-805.418852	-22.541971	1.076032
-808.646445	-30.061625	1.081037
-812.929713	-23.810742	1.086042
-816.656124	-37.077061	1.091046
-821.073483	-16.170111	1.096051
-824.633553	-23.926739	1.101056
-827.944690	-30.871657	1.106061
-831.802067	-21.748018	1.111066
-835.356658	-34.907741	1.116070
-839.150370	-29.282231	1.121075
-842.934016	-25.328193	1.126080
-846.807733	-32.184729	1.131085
-850.997894	-24.898491	1.136090
-854.281636	-29.646486	1.141094
-857.749359	-38.201502	1.146099
-862.177106	-29.831827	1.151104
-865.719932	-36.359630	1.156109
-869.895344	-22.440395	1.161114
-873.235507	-22.581291	1.166118
-877.075076	-28.588590	1.171123
-881.027885	-24.872357	1.176128
-884.442109	-30.521896	1.181133
-888.494225	-36.794791	1.186138
-891.745664	-32.960453	1.191142
-895.623943	-20.870502	1.196147
-899.428678	-26.236831	1.201152
-903.537773	-20.962890	1.206157
-907.003713	-25.278010	1.211162
-910.390994	-29.263527	1.216166
-914.365058	-29.508003	1.221171
-918.657834	-26.527348	1.226176
-922.480513	-36.525081	1.231181
-926.029402	-22.753233	1.236186
-929.402140	-37.033043	1.241190
-933.652661	-21.789770	1.246195
-937.299259	-25.107782	1.251200
-940.641171	-29.616132	1.256205
-944.412460	-19.044358	1.261210
-948.463588	-37.261824	1.266214
-952.814170	-24.066597	1.271219
-956.244009	-31.090107	1.276224
-959.793397	-43.115126	1.281229
-963.524494	-31.690386	1.286234
-967.160405	-30.399396	1.291238
-971.169820	-31.565301	1.296243
-974.783347	-27.330777	1.301248
-978.243429	-42.395991	1.306253
-982.170271	-28.142619	1.311258
-985.835798	-35.932576	1.316262
-989.930355	-31.343585	1.321267
-993.508130	-32.985300	1.326272
-997.646117	-30.371429	1.331277
-1001.435836	-24.568122	1.336282
-1004.816882	-28.032564	1.341286
-1008.792681	-34.483016	1.346291
-1012.616761	-29.651834	1.351296
-1016.147500	-32.206138	1.356301
-1020.156764	-25.128301	1.361306
-1023.563802	-33.465701	1.366310
-1027.460407	-21.495612	1.371315
-1031.124644	-35.302896	1.376320
-1034.763027	-35.797957	1.381325
-1038.591521	-35.239244	1.386330
-1042.406850	-30.112970	1.391334
-1046.248875	-28.162891	1.396339
-1050.411278	-32.134604	1.401344
-1054.021066	-27.652997	1.406349
-1057.643308	-36.990323	1.411354
-1060.873475	-36.820562	1.416358
-1064.961152	-23.105840	1.421363
-1069.005840	-34.179477	1.426368
-1072.516738	-24.227861	1.431373
-1076.194612	-22.655622	1.436378
-1080.047412	-30.774990	1.441382
-1083.816869	-31.195397	1.446387
-1087.957133	-25.450993	1.451392
-1091.345247	-29.235849	1.456397
-1095.114482	-24.608835	1.461402
-1098.975458	-34.041938	1.466406
-1102.426021	-26.665437	1.471411
-1106.653337	-21.853174	1.476416
-1110.276889	-32.957834	1.481421
-1113.905808	-32.120287	1.486426
-1117.496687	-46.199323	1.491430
-1121.189703	-33.041201	1.496435
-1125.379220	-31.032251	1.501440
-1129.192646	-36.913998	1.506445
-1132.952733	-27.384447	1.511450
-1136.365834	-34.000378	1.516454
-1140.364872	-36.548953	1.521459
-1143.856454	-29.711417	1.526464
-1148.048825	-35.590851	1.531469
-1151.552774	-36.432063	1.536474
-1155.340081	-33.257480	1.541478
-1158.947976	-37.965782	1.546483
-1162.950393	-31.856983	1.551488
-1166.969321	-39.430838	1.556493
-1170.491953	-25.740124	1.561498
-1173.785526	-42.944606	1.566502
-1177.678807	-30.096532	1.571507
-1181.504113	-38.628515	1.576512
-1185.392195	-34.505855	1.581517
-1189.374480	-26.008180	1.586522
-1193.241012	-35.933774	1.591526
-1196.840513	-39.531693	1.596531
-1200.084996	-42.555680	1.601536
-1204.076687	-30.026106	1.606541
-1207.987695	-31.406027	1.611546
-1211.872087	-27.968256	1.616550
-1215.611721	-39.552437	1.621555
-1219.251181	-29.001353	1.626560
-1222.971557	-46.342445	1.631565
-1226.980942	-30.183301	1.636570
-1230.610782	-28.840840	1.641574
-1234.215545	-31.318312	1.646579
-1238.252642	-34.574929	1.651584
-1241.922858	-31.078350	1.656589
-1246.029812	-26.499551	1.661594
-1249.158456	-37.880274	1.666598
-1252.784628	-30.175865	1.671603
-1257.196114	-31.262740	1.676608
-1260.532823	-36.681275	1.681613
-1264.562202	-32.106977	1.686618
-1267.868558	-46.775294	1.691622
-1271.442418	-32.486518	1.696627
-1275.793294	-34.525999	1.701632
-1279.918570	-39.338949	1.706637
-1283.598963	-28.259290	1.711642
-1287.101520	-39.955399	1.716646
-1290.827826	-37.914641	1.721651
-1294.315669	-27.879681	1.726656
-1297.749009	-31.065678	1.731661
-1302.210224	-22.358714	1.736666
-1305.943272	-26.406561	1.741670
-1309.410072	-14.828072	1.746675
-1313.127563	-26.333643	1.751680
-1316.801147	-39.850372	1.756685
-1321.145850	-25.748778	1.761690
-1324.714396	-26.883717	1.766694
-1328.671246	-24.626238	1.771699
-1332.372194	-29.965869	1.776704
-1335.827937	-35.226479	1.781709
-1339.402053	-35.772345	1.786714
-1343.149468	-29.691448	1.791718
-1346.916636	-29.919420	1.796723
-1350.906938	-29.294873	1.801728
-1354.669527	-33.673772	1.806733
-1358.530609	-22.142486	1.811738
-1362.068532	-36.478730	1.816742
-1365.961681	-35.470771	1.821747
-1369.890402	-28.920875	1.826752
-1373.567926	-37.529792	1.831757
-1377.677023	-24.265265	1.836762
-1381.093254	-26.788453	1.841766
-1384.711899	-31.884149	1.846771
-1388.379494	-20.889952	1.851776
-1392.048751	-35.118395	1.856781
-1396.178086	-29.077192	1.861786
-1400.090707	-23.616255	1.866790
-1403.832468	-29.362362	1.871795
-1407.560958	-28.352312	1.876800
-1410.640514	-26.589930	1.881805
-1414.817772	-24.624999	1.886810
-1418.171567	-26.776535	1.891814
-1422.262360	-26.854809	1.896819
-1426.043851	-29.596972	1.901824
-1429.929906	-28.982671	1.906829
-1433.933996	-30.055590	1.911834
-1437.470710	-27.149315	1.916838
-1441.299758	-28.677567	1.921843
-1445.021369	-19.383915	1.926848
-1448.487082	-26.550715	1.931853
-1452.497976	-23.670989	1.936858
-1456.263618	-28.394555	1.941862
-1459.984985	-28.483031	1.946867
-1463.636264	-23.035452	1.951872
-1467.497784	-27.472433	1.956877
-1471.437275	-23.922919	1.961882
-1475.075580	-35.190165	1.966886
-1478.762905	-24.154834	1.971891
-1482.583851	-28.722855	1.976896
-1486.225445	-30.866049	1.981901
-1490.148006	-30.231610	1.986906
-1493.614944	-32.388568	1.991910
-1497.834403	-22.799092	1.996915
-1501.698990	-23.836078	2.006912
-1502.269832	-27.627007	2.016909
-1500.061420	-28.288489	2.026906
-1497.187200	-31.462743	2.036902
-1495.029489	-37.703624	2.046899
-1493.210029	-29.053955	2.056896
-1491.230068	-28.062110	2.066893
-1489.273624	-22.948874	2.076890
-1487.507599	-24.248406	2.086886
-1485.566521	-28.537877	2.096883
-1483.594824	-28.188871	2.106880
-1481.887087	-35.736019	2.116877
-1480.146830	-20.895638	2.126874
-1477.956650	-32.173482	2.136870
-1475.963919	-34.371353	2.146867
-1473.956463	-33.338110	2.156864
-1472.109006	-39.922424	2.166861
-1470.520767	-31.279920	2.176858
-1468.710534	-28.734138	2.186854
-1466.503454	-38.598451	2.196851
-1464.574308	-29.161109	2.206848
-1462.833772	-30.151823	2.216845
-1460.962141	-33.042351	2.226842
-1459.219006	-30.607388	2.236838
-1457.129947	-35.021575	2.246835
-1455.469805	-33.034344	2.256832
-1453.358803	-37.813595	2.266829
-1451.258900	-35.435751	2.276826
-1449.401770	-29.442952	2.286822
-1447.932722	-36.471892	2.296819
-1445.970302	-35.718763	2.306816
-1444.327848	-32.201950	2.316813
-1441.777464	-32.108182	2.326810
-1440.171693	-31.215845	2.336806
-1438.489366	-33.348199	2.346803
-1436.769737	-37.316403	2.356800
-1434.499086	-36.975748	2.366797
-1432.572821	-29.691457	2.376794
-1430.775074	-30.449744	2.386790
-1428.885653	-30.404866	2.396787
-1427.027482	-20.616668	2.406784
-1425.094507	-28.177740	2.416781
-1423.172352	-30.231645	2.426778
-1421.384514	-27.912750	2.436774
-1419.494403	-27.477999	2.446771
-1417.762858	-30.878136	2.456768
-1416.119914	-25.100473	2.466765
-1414.053069	-28.751644	2.476762
-1411.823098	-29.296501	2.486758
-1409.918420	-22.774470	2.496755
-1408.255153	-39.125982	2.506752
-1406.387859	-37.825520	2.516749
-1404.599197	-30.309188	2.526746
-1402.473111	-32.321519	2.536742
-1400.470740	-31.472121	2.546739
-1398.988738	-32.945575	2.556736
-1396.839683	-33.168010	2.566733
-1395.265686	-26.971952	2.576730
-1393.416611	-32.995981	2.586726
-1391.179552	-30.347949	2.596723
-1389.544248	-29.461884	2.606720
-1387.404737	-33.195712	2.616717
-1385.588707	-35.137866	2.626714
-1383.835599	-32.822855	2.636710
-1382.182848	-25.418946	2.646707
-1380.044884	-32.689134	2.656704
-1378.126423	-28.074948	2.666701
-1376.476367	-24.976114	2.676698
-1374.481753	-28.738838	2.686694
-1372.328443	-29.898187	2.696691
-1370.677906	-27.408860	2.706688
-1368.914972	-34.797413	2.716685
-1367.187917	-26.668066	2.726682
-1365.238649	-28.326817	2.736678
-1362.958773	-33.878240	2.746675
-1360.974336	-26.751605	2.756672
-1359.418768	-28.386801	2.766669
-1357.742782	-27.739315	2.776666
-1355.676113	-29.634731	2.786662
-1353.719503	-20.267986	2.796659
-1351.632502	-33.422247	2.806656
-1350.171426	-30.247357	2.816653
-1348.363130	-25.713399	2.826650
-1346.240031	-24.153851	2.836646
-1344.407272	-27.429621	2.846643
-1342.593291	-30.165574	2.856640
-1340.593886	-34.279540	2.866637
-1338.778287	-32.089752	2.876634
-1336.741636	-24.480430	2.886630
-1335.041153	-32.525237	2.896627
-1333.273721	-21.648816	2.906624
-1331.041677	-24.323791	2.916621
-1329.358214	-29.555525	2.926618
-1327.513226	-27.886713	2.936614
-1325.637176	-25.834475	2.946611
-1323.583055	-38.287176	2.956608
-1321.790901	-40.305981	2.966605
-1320.375753	-25.350267	2.976602
-1318.151189	-33.355796	2.986598
-1316.294910	-35.166980	2.996595
-1314.242677	-38.446275	3.006592
-1312.448877	-31.811683	3.016589
-1310.471787	-25.684813	3.026586
-1308.895511	-22.474651	3.036582
-1306.660448	-25.407439	3.046579
-1304.815873	-32.321152	3.056576
-1303.278073	-24.194617	3.066573
-1301.201596	-24.975311	3.076570
-1299.274107	-29.739271	3.086566
-1297.466086	-27.298777	3.096563
-1295.645692	-31.409318	3.106560
-1293.863488	-29.893052	3.116557
-1291.922546	-29.333709	3.126554
-1289.928404	-32.736310	3.136550
-1287.986331	-32.581330	3.146547
-1286.005321	-29.366459	3.156544
-1284.387289	-29.368023	3.166541
-1282.408212	-27.998510	3.176538
-1280.622079	-24.850334	3.186534
-1278.786119	-25.417264	3.196531
-1276.771962	-30.856613	3.206528
-1274.935688	-24.516134	3.216525
-1273.248267	-21.208478	3.226522
-1271.002123	-30.221568	3.236518
-1269.403818	-29.220554	3.246515
-1267.344787	-29.455302	3.256512
-1265.383657	-21.153341	3.266509
-1263.751764	-25.936281	3.276506
-1261.669209	-19.106286	3.286502
-1259.972823	-26.673581	3.296499
-1258.259152	-22.694368	3.306496
-1255.864887	-23.432725	3.316493
-1254.088044	-20.218306	3.326490
-1252.598985	-18.765614	3.336486
-1250.602854	-23.002136	3.346483
-1248.684521	-18.776209	3.356480
-1247.008114	-22.560536	3.366477
-1245.012146	-22.764648	3.376474
-1242.793424	-21.076630	3.386470
-1240.810902	-21.482258	3.396467
-1239.225049	-19.266674	3.406464
-1237.643935	-23.218892	3.416461
-1235.472992	-21.921091	3.426458
-1233.713473	-19.990645	3.436454
-1231.660075	-16.869406	3.446451
-1229.564460	-22.921718	3.456448
-1228.188641	-19.745733	3.466445
-1226.122926	-15.683887	3.476442
-1224.347578	-19.286675	3.486438
-1222.601143	-22.839049	3.496435
-1220.520270	-25.786554	3.506432
-1218.314938	-23.824808	3.516429
-1216.801368	-22.358648	3.526426
-1214.829346	-20.820589	3.536422
-1212.944101	-25.231956	3.546419
-1211.447191	-21.538528	3.556416
-1209.073567	-20.041042	3.566413
-1207.339519	-13.014709	3.576410
-1205.662949	-19.846216	3.586406
-1203.675994	-19.980959	3.596403
-1201.825110	-18.306671	3.606400
-1199.582579	-22.315751	3.616397
-1198.219196	-25.342635	3.626394
-1196.192627	-17.180542	3.636390
-1194.222945	-18.899258	3.646387
-1192.297604	-26.395780	3.656384
-1190.402708	-29.090886	3.666381
-1188.903327	-22.642747	3.676378
-1186.559645	-20.147350	3.686374
-1185.153658	-20.580678	3.696371
-1182.741183	-16.339024	3.706368
-1180.669963	-15.814640	3.716365
-1179.277022	-21.936053	3.726362
-1177.499888	-18.707409	3.736358
-1175.286129	-21.049335	3.746355
-1173.733047	-22.668224	3.756352
-1171.841295	-26.253283	3.766349
-1169.994849	-25.651877	3.776346
-1167.872616	-26.640288	3.786342
-1166.007848	-24.500853	3.796339
-1164.094045	-21.153548	3.806336
-1162.336268	-22.345733	3.816333
-1160.542891	-19.017050	3.826330
-1158.478957	-20.278739	3.836326
-1156.662207	-15.763337	3.846323
-1154.783240	-27.578463	3.856320
-1153.025954	-22.957238	3.866317
-1151.072721	-23.056544	3.876314
-1149.102368	-25.923153	3.886310
-1147.521014	-22.408970	3.896307
-1145.397881	-25.394749	3.906304
-1143.515561	-22.553937	3.916301
-1141.879242	-30.392579	3.926298
-1139.794706	-29.530837	3.936294
-1137.959427	-23.458484	3.946291
-1136.220245	-21.477344	3.956288
-1134.164114	-24.911840	3.966285
-1132.192671	-27.803870	3.976282
-1130.481605	-25.710867	3.986278
-1128.418136	-24.291567	3.996275
-1126.598072	-24.129564	4.006272
-1124.664247	-17.324586	4.016269
-1123.103959	-17.943604	4.026266
-1121.330862	-17.115701	4.036262
-1119.004789	-16.439411	4.046259
-1117.233317	-21.582460	4.056256
-1115.295725	-27.569925	4.066253
-1113.652638	-26.834897	4.076250
-1111.834741	-21.844410	4.086246
-1109.783635	-25.574906	4.096243
-1107.997918	-26.533114	4.106240
-1106.009143	-20.963678	4.116237
-1104.149372	-20.798535	4.126234
-1102.106859	-23.495081	4.136230
-1100.241243	-11.397910	4.146227
-1098.437036	-18.243450	4.156224
-1096.987396	-17.545356	4.166221
-1094.812907	-16.660069	4.176218
-1093.080098	-24.809364	4.186214
-1091.112641	-19.455964	4.196211
-1089.131851	-25.732933	4.206208
-1087.072095	-22.516270	4.216205
-1085.321098	-16.653005	4.226202
-1083.661005	-21.598226	4.236198
-1081.588717	-25.052630	4.246195
-1079.713812	-22.906851	4.256192
-1077.775891	-19.980146	4.266189
-1075.835051	-22.649355	4.276186
-1073.982538	-22.983523	4.286182
-1072.499887	-23.149590	4.296179
-1070.589771	-25.425483	4.306176
-1068.435057	-26.764767	4.316173
-1066.674034	-25.949102	4.326170
-1064.623464	-26.520192	4.336166
-1063.148767	-25.429794	4.346163
-1060.748756	-24.280564	4.356160
-1059.112302	-28.238361	4.366157
-1057.229220	-22.130955	4.376154
-1055.433647	-17.387886	4.386150
-1053.558854	-19.347083	4.396147
-1051.346061	-26.619493	4.406144
-1049.656062	-26.244007	4.416141
-1048.106561	-24.928735	4.426138
-1046.238191	-24.297581	4.436134
-1044.347006	-24.082155	4.446131
-1041.961554	-22.253250	4.456128
-1040.245588	-29.353036	4.466125
-1038.513727	-31.260940	4.476122
-1036.564016	-23.294813	4.486118
-1034.901480	-21.209763	4.496115
-1032.812097	-24.969999	4.506112
-1030.856854	-27.685683	4.516109
-1029.138773	-18.264692	4.526106
-1027.019117	-25.100632	4.536102
-1025.340840	-27.178368	4.546099
-1023.518522	-18.396111	4.556096
-1021.624100	-24.997090	4.566093
-1019.960457	-25.506261	4.576090
-1018.131126	-24.791477	4.586086
-1015.874690	-22.907177	4.596083
-1014.171142	-30.145477	4.606080
-1011.792797	-32.513571	4.616077
-1010.436557	-22.813662	4.626074
-1008.482378	-22.167781	4.636070
-1006.751680	-32.612330	4.646067
-1004.382658	-29.171909	4.656064
-1002.810113	-35.107222	4.666061
-1000.791918	-31.342289	4.676058
-999.071805	-23.149948	4.686054
-997.327043	-26.676631	4.696051
-995.542205	-32.388537	4.706048
-993.535357	-36.846021	4.716045
-991.383492	-26.973352	4.726042
-989.478448	-24.554441	4.736038
-987.964777	-26.318477	4.746035
-985.812900	-40.695390	4.756032
-984.302608	-31.177988	4.766029
-982.125457	-32.560253	4.776026
-980.179404	-28.681139	4.786022
-978.431832	-29.971024	4.796019
-976.790766	-27.089915	4.806016
-974.560856	-25.324483	4.816013
-972.632994	-22.958151	4.826010
-971.037789	-30.929053	4.836006
-969.292945	-26.671986	4.846003
-967.146203	-31.562321	4.856000
-965.413330	-34.686051	4.865997
-963.350623	-29.178833	4.875994
-961.380347	-29.860144	4.885990
-960.030092	-26.105203	4.895987
-957.844994	-25.477258	4.905984
-955.664751	-27.188395	4.915981
-954.115237	-30.216486	4.925978
-952.120052	-29.405020	4.935974
-950.387317	-28.346337	4.945971
-948.231522	-33.050220	4.955968
-946.365501	-25.372189	4.965965
-944.709208	-31.513479	4.975962
-942.948644	-28.570932	4.985958
-941.108371	-30.530836	4.995955
-939.276544	-25.749263	5.005952
-936.894555	-36.354742	5.015949
-935.285347	-25.833176	5.025946
-933.402439	-31.254422	5.035942
-931.563555	-23.581512	5.045939
-929.702108	-23.228615	5.055936
-927.684601	-23.942712	5.065933
-925.740541	-23.074104	5.075930
-924.064044	-28.926524	5.085926
-922.259635	-17.588308	5.095923
-920.007138	-24.180152	5.105920
-918.681673	-29.745931	5.115917
-916.721847	-26.942583	5.125914
-914.573776	-26.382884	5.135910
-912.785522	-18.408193	5.145907
-910.926181	-24.196687	5.155904
-909.130541	-23.675367	5.165901
-906.890530	-24.406074	5.175898
-905.284670	-19.201524	5.185894
-903.503541	-20.964061	5.195891
-901.533200	-25.193018	5.205888
-899.393585	-23.623065	5.215885
-897.585326	-21.235968	5.225882
-895.925904	-21.382819	5.235878
-893.969538	-24.993783	5.245875
-892.021963	-24.997237	5.255872
-890.797197	-23.912557	5.265869
-888.278538	-24.297818	5.275866
-886.344850	-15.323255	5.285862
-884.730081	-18.338055	5.295859
-882.917889	-20.369212	5.305856
-880.837513	-22.489027	5.315853
-879.036426	-24.687342	5.325850
-876.999609	-16.826563	5.335846
-875.062247	-21.692823	5.345843
-873.345359	-19.403198	5.355840
-871.382739	-24.636629	5.365837
-869.832359	-22.517740	5.375834
-867.532829	-22.086414	5.385830
-865.897096	-27.218638	5.395827
-863.899123	-21.179953	5.405824
-862.103985	-27.416015	5.415821
-860.182217	-24.169191	5.425818
-858.569906	-20.508180	5.435814
-856.552660	-20.312754	5.445811
-854.364432	-20.468324	5.455808
-852.838984	-21.738398	5.465805
-850.882393	-23.451580	5.475802
-848.895732	-20.654041	5.485798
-846.996364	-19.765592	5.495795
-844.983761	-18.353695	5.505792
-843.478260	-23.394039	5.515789
-841.147155	-20.042115	5.525786
-839.914408	-18.093471	5.535782
-837.958254	-18.838734	5.545779
-835.815638	-18.950683	5.555776
-833.705048	-21.735249	5.565773
-832.049994	-23.745985	5.575770
-830.272293	-29.721884	5.585766
-828.276866	-23.845382	5.595763
-826.516620	-25.260333	5.605760
-824.570680	-22.419951	5.615757
-822.894888	-22.717779	5.625754
-820.830036	-19.335906	5.635750
-818.849078	-27.924137	5.645747
-817.131034	-24.998377	5.655744
-815.277988	-26.426574	5.665741
-813.553432	-18.648447	5.675738
-811.441446	-19.320708	5.685734
-809.517310	-17.264675	5.695731
-807.699260	-20.422436	5.705728
-805.804761	-20.977829	5.715725
-803.615123	-15.827040	5.725722
-801.953513	-18.626654	5.735718
-800.524625	-17.884008	5.745715
-798.262129	-19.229224	5.755712
-796.553560	-14.948851	5.765709
-794.731202	-12.143948	5.775706
-792.679962	-15.512644	5.785702
-790.599735	-18.805450	5.795699
-788.780090	-17.863161	5.805696
-787.081100	-22.067605	5.815693
-785.307277	-15.102545	5.825690
-783.113701	-17.818231	5.835686
-781.457890	-17.525502	5.845683
-779.759525	-10.867304	5.855680
-777.807330	-12.742347	5.865677
-775.618111	-23.308987	5.875674
-773.941057	-12.322890	5.885670
-771.899440	-16.469987	5.895667
-769.858186	-20.017057	5.905664
-768.336206	-21.805968	5.915661
-766.590586	-24.208480	5.925658
-764.442457	-19.840449	5.935654
-762.683145	-20.928380	5.945651
-760.806477	-33.734393	5.955648
-758.976866	-17.935053	5.965645
-757.082736	-25.366271	5.975642
-755.252832	-23.359867	5.985638
-753.027517	-23.306546	5.995635
-751.564271	-18.832206	6.005632
-749.644914	-19.135751	6.015629
-747.646471	-18.329366	6.025626
-745.679676	-14.707555	6.035622
-743.985827	-17.570700	6.045619
-742.021260	-21.476523	6.055616
-740.095868	-8.722290	6.065613
-738.169007	-20.131136	6.075610
-736.335059	-16.508612	6.085606
-734.924546	-20.993745	6.095603
-732.825746	-24.114215	6.105600
-730.660066	-22.260919	6.115597
-728.894772	-14.599750	6.125594
-726.906980	-22.805346	6.135590
-725.135299	-18.636052	6.145587
-723.051966	-17.615856	6.155584
-721.384744	-26.089148	6.165581
-719.552692	-25.330356	6.175578
-717.620854	-23.041807	6.185574
-715.683892	-18.701560	6.195571
-713.764497	-23.122744	6.205568
-711.736875	-27.799628	6.215565
-710.207468	-25.119942	6.225562
-708.533882	-23.434292	6.235558
-706.497858	-15.061673	6.245555
-704.353466	-27.910434	6.255552
-702.660928	-23.060620	6.265549
-700.771617	-20.691055	6.275546
-698.646376	-22.699468	6.285542
-696.940630	-16.978649	6.295539
-695.241117	-29.876308	6.305536
-693.237004	-27.804540	6.315533
-691.191705	-23.336329	6.325530
-689.670991	-25.432864	6.335526
-687.703794	-22.270516	6.345523
-685.619716	-17.780075	6.355520
-683.511976	-22.209228	6.365517
-682.161095	-22.196108	6.375514
-680.292513	-19.720588	6.385510
-678.308855	-18.062355	6.395507
-676.367417	-22.032322	6.405504
-674.231395	-21.427847	6.415501
-672.546004	-13.689132	6.425498
-670.572705	-20.589812	6.435494
-669.091009	-13.292204	6.445491
-666.959830	-12.494328	6.455488
-664.966430	-24.057428	6.465485
-663.235701	-23.729221	6.475482
-661.374492	-15.767550	6.485478
-659.326038	-20.185631	6.495475
-657.585101	-25.430843	6.505472
-655.731433	-21.803511	6.515469
-654.052058	-15.574789	6.525466
-652.013881	-18.908125	6.535462
-650.020104	-19.687665	6.545459
-648.138481	-17.919952	6.555456
-646.114646	-21.377300	6.565453
-644.303646	-23.731754	6.575450
-642.710082	-18.026125	6.585446
-640.841953	-22.535374	6.595443
-638.799604	-19.645502	6.605440
-636.603755	-26.837484	6.615437
-635.267730	-28.001372	6.625434
-633.418348	-21.051418	6.635430
-630.947617	-20.462486	6.645427
-629.505519	-25.798875	6.655424
-627.559119	-27.598664	6.665421
-625.757279	-24.228276	6.675418
-624.121959	-26.431497	6.685414
-621.785807	-25.794215	6.695411
-620.145324	-14.961613	6.705408
-618.044220	-19.909096	6.715405
-616.297945	-12.824237	6.725402
-614.552107	-11.153217	6.735398
-612.436158	-18.894494	6.745395
-610.609168	-16.630154	6.755392
-608.781852	-14.820576	6.765389
-606.841334	-24.340036	6.775386
-605.018492	-25.449053	6.785382
-603.286485	-14.812628	6.795379
-601.390940	-23.304956	6.805376
-599.608334	-23.237606	6.815373
-597.540334	-17.860353	6.825370
-595.311272	-22.943515	6.835366
-593.900011	-15.178313	6.845363
-592.095396	-16.510186	6.855360
-590.072329	-21.116777	6.865357
-587.894941	-23.515508	6.875354
-586.045719	-17.718054	6.885350
-584.619692	-27.278460	6.895347
-582.695519	-23.703382	6.905344
-580.581515	-21.581178	6.915341
-578.577323	-24.211167	6.925338
-577.101975	-22.777950	6.935334
-575.237875	-20.944224	6.945331
-573.161251	-17.024035	6.955328
-571.088562	-26.656155	6.965325
-569.361586	-24.811573	6.975322
-567.538806	-25.011129	6.985318
-565.726897	-19.706618	6.995315
-563.807069	-23.788302	7.005312
-562.159944	-18.209585	7.015309
-559.917745	-20.244455	7.025306
-558.028400	-19.587841	7.035302
-556.385965	-19.019674	7.045299
-554.261909	-18.008991	7.055296
-552.501135	-21.774751	7.065293
-550.640513	-17.793199	7.075290
-549.026209	-20.932436	7.085286
-547.047291	-18.761783	7.095283
-544.866884	-17.280118	7.105280
-542.934589	-16.534042	7.115277
-541.184154	-19.074526	7.125274
-539.570933	-20.393157	7.135270
-537.574731	-12.385047	7.145267
-535.556644	-21.586865	7.155264
-533.872271	-13.173703	7.165261
-531.750295	-19.452271	7.175258
-530.078613	-19.867651	7.185254
-528.007528	-13.775601	7.195251
-526.069497	-18.886425	7.205248
-524.453353	-20.672857	7.215245
-522.693689	-22.131702	7.225242
-520.906420	-16.447448	7.235238
-518.632628	-23.654940	7.245235
-516.721449	-22.120776	7.255232
-515.094414	-20.653328	7.265229
-512.945823	-23.964712	7.275226
-511.143852	-17.101810	7.285222
-509.514047	-18.502014	7.295219
-507.273773	-24.778928	7.305216
-505.331006	-20.682571	7.315213
-503.892113	-17.784616	7.325210
-501.899672	-24.026682	7.335206
-499.884646	-19.171375	7.345203
-498.350776	-19.375261	7.355200
-496.163384	-29.658764	7.365197
-494.599194	-23.119435	7.375194
-492.288192	-23.592684	7.385190
-490.608000	-27.552362	7.395187
-488.721881	-18.001449	7.405184
-486.622726	-25.274174	7.415181
-484.851808	-17.296352	7.425178
-482.963823	-12.889662	7.435174
-481.461838	-14.646782	7.445171
-479.349227	-17.652409	7.455168
-477.380485	-25.343224	7.465165
-475.648617	-22.863072	7.475162
-473.562712	-20.748914	7.485158
-471.827264	-18.719306	7.495155
-470.123965	-21.792183	7.505152
-467.988437	-23.743620	7.515149
-466.060024	-23.915760	7.525146
-464.334043	-26.970149	7.535142
-462.516609	-18.014528	7.545139
-460.380170	-18.706172	7.555136
-458.838254	-18.140832	7.565133
-456.996753	-22.277819	7.575130
-454.629992	-18.075450	7.585126
-452.889596	-13.359392	7.595123
-451.242663	-16.326945	7.605120
-449.331758	-20.187657	7.615117
-447.281876	-20.371284	7.625114
-445.550759	-19.806149	7.635110
-443.823270	-12.484478	7.645107
-442.296175	-13.642458	7.655104
-439.938697	-18.218649	7.665101
-437.608472	-14.488823	7.675098
-436.243646	-18.173910	7.685094
-434.466500	-19.794949	7.695091
-432.386508	-18.717122	7.705088
-430.433794	-20.617232	7.715085
-428.454503	-19.891197	7.725082
-426.922939	-17.748478	7.735078
-425.016520	-21.608454	7.745075
-423.265117	-20.714982	7.755072
-420.908866	-20.453321	7.765069
-418.992590	-18.299398	7.775066
-417.587092	-23.315634	7.785062
-415.858264	-26.018359	7.795059
-413.752234	-19.857577	7.805056
-411.761606	-28.571783	7.815053
-409.794964	-16.813774	7.825050
-408.112823	-26.981800	7.835046
-406.132405	-16.421187	7.845043
-404.201985	-26.789897	7.855040
-402.321011	-24.644534	7.865037
-400.550372	-26.711327	7.875034
-398.259715	-25.616583	7.885030
-396.986051	-19.117633	7.895027
-394.945159	-16.652024	7.905024
-392.806584	-22.541570	7.915021
-391.380078	-24.665510	7.925018
-389.303542	-27.087435	7.935014
-387.225053	-26.295103	7.945011
-385.685667	-31.580578	7.955008
-383.632383	-25.573972	7.965005
-381.739650	-23.642037	7.975002
-379.898018	-27.521633	7.984998
-378.130385	-23.338788	7.994995
-376.135466	-23.020973	8.004992
-374.216598	-25.002471	8.014989
-372.313209	-27.980917	8.024986
-370.332842	-32.422626	8.034982
-368.668132	-27.645479	8.044979
-366.635551	-22.927060	8.054976
-364.843846	-27.993874	8.064973
-363.516135	-31.837195	8.074970
-361.180463	-28.125533	8.084966
-359.031988	-31.013629	8.094963
-357.333225	-31.063759	8.104960
-355.369934	-26.430580	8.114957
-353.522069	-28.154423	8.124954
-351.573139	-32.297430	8.134950
-350.044861	-27.455859	8.144947
-348.156518	-26.694713	8.154944
-346.121310	-19.338412	8.164941
-343.962804	-29.692968	8.174938
-342.491357	-24.359185	8.184934
-340.423167	-26.411861	8.194931
-338.589984	-25.165085	8.204928
-336.792730	-29.471752	8.214925
-334.800479	-30.261840	8.224922
-332.974756	-29.842772	8.234918
-331.125787	-20.498936	8.244915
-329.264967	-27.847166	8.254912
-327.555833	-23.408640	8.264909
-325.368296	-25.819811	8.274906
-323.564687	-21.096379	8.284902
-321.714683	-27.819226	8.294899
-319.853687	-24.199105	8.304896
-317.925159	-23.611710	8.314893
-315.926890	-29.401427	8.324890
-314.237264	-29.445332	8.334886
-312.202443	-24.360926	8.344883
-310.629125	-27.007176	8.354880
-308.973272	-27.239886	8.364877
-306.790760	-20.333357	8.374874
-304.685099	-30.497876	8.384870
-303.067626	-31.281794	8.394867
-301.033616	-30.828059	8.404864
-299.112081	-30.247427	8.414861
-297.181461	-27.456254	8.424858
-295.478058	-24.717227	8.434854
-293.361306	-17.091275	8.444851
-291.905342	-26.634213	8.454848
-289.896152	-25.072880	8.464845
-288.122213	-27.337477	8.474842
-285.953175	-17.861541	8.484838
-284.198760	-26.004293	8.494835
-282.315290	-16.392775	8.504832
-280.353371	-22.647168	8.514829
-278.674028	-22.335740	8.524826
-276.632304	-28.080262	8.534822
-274.680624	-23.593572	8.544819
-272.926684	-17.302250	8.554816
-271.000263	-27.164993	8.564813
-269.045042	-26.686024	8.574810
-267.316962	-23.998280	8.584807
-265.443163	-21.420630	8.594803
-263.791526	-27.868630	8.604800
-261.602683	-23.260317	8.614797
-259.333966	-30.517294	8.624794
-257.732809	-25.330466	8.634791
-256.415297	-20.627285	8.644787
-254.309916	-24.217325	8.654784
-252.496768	-21.401049	8.664781
-250.083988	-26.025359	8.674778
-248.558271	-31.408042	8.684775
-246.534279	-26.727618	8.694771
-245.034793	-24.177048	8.704768
-242.843448	-22.875261	8.714765
-240.970431	-27.156061	8.724762
-239.057123	-28.688169	8.734759
-237.451873	-29.320100	8.744755
-235.803454	-20.539406	8.754752
-233.311210	-27.388375	8.764749
-231.605856	-26.321630	8.774746
-229.355965	-22.648245	8.784743
-227.776272	-29.741548	8.794739
-226.084142	-30.598906	8.804736
-224.280128	-30.506274	8.814733
-222.398957	-34.471007	8.824730
-220.240702	-41.307706	8.834727
-218.539280	-34.022755	8.844723
-216.565076	-36.575037	8.854720
-214.793802	-32.046876	8.864717
-212.898248	-28.163778	8.874714
-210.814681	-34.415424	8.884711
-209.290387	-28.354236	8.894707
-207.234581	-26.793956	8.904704
-205.477192	-34.144538	8.914701
-203.105187	-29.617504	8.924698
-201.965643	-31.580283	8.934695
-200.332013	-29.136351	8.944691
-197.836573	-33.658545	8.954688
-195.855297	-29.275980	8.964685
-193.994508	-34.846305	8.974682
-192.347467	-30.492502	8.984679
-190.320678	-31.164831	8.994675
-188.469326	-27.220976	9.004672
-186.610979	-31.382558	9.014669
-184.873246	-41.644574	9.024666
-182.796996	-33.672605	9.034663
-180.861158	-37.369730	9.044659
-179.458461	-31.750147	9.054656
-177.261010	-35.556908	9.064653
-175.395505	-29.468044	9.074650
-173.479326	-31.423695	9.084647
-171.768730	-28.515207	9.094643
-169.672937	-28.980646	9.104640
-167.953891	-32.665272	9.114637
-165.874413	-32.851804	9.124634
-163.945296	-34.569523	9.134631
-162.153211	-35.941708	9.144627
-160.512912	-37.930691	9.154624
-158.755010	-26.696484	9.164621
-156.703203	-27.671184	9.174618
-154.605416	-38.148522	9.184615
-153.041008	-34.196747	9.194611
-151.027522	-37.088386	9.204608
-148.987605	-28.452198	9.214605
-147.398123	-40.302560	9.224602
-145.440836	-40.115910	9.234599
-143.480288	-26.420995	9.244595
-141.776039	-32.924679	9.254592
-139.690439	-34.386310	9.264589
-137.712936	-37.659019	9.274586
-135.740769	-34.028070	9.284583
-134.033132	-30.787520	9.294579
-132.385188	-27.869007	9.304576
-130.536421	-18.749161	9.314573
-128.445079	-28.638119	9.324570
-126.519601	-26.450690	9.334567
-124.699300	-26.838979	9.344563
-122.758538	-26.864400	9.354560
-120.968856	-29.867142	9.364557
-119.013346	-23.926793	9.374554
-117.230905	-31.833920	9.384551
-115.255529	-20.320174	9.394547
-113.635586	-27.383521	9.404544
-111.678295	-21.519234	9.414541
-109.481472	-26.314209	9.424538
-107.897745	-27.487331	9.434535
-105.982882	-25.936054	9.444531
-104.113194	-19.713590	9.454528
-102.200287	-16.339981	9.464525
-100.441188	-25.351743	9.474522
-98.366770	-24.819024	9.484519
-96.578229	-28.037873	9.494515
-94.744518	-22.332267	9.504512
-92.985341	-30.080939	9.514509
-90.853996	-32.156112	9.524506
-89.129556	-27.699323	9.534503
-87.300723	-32.855548	9.544499
-85.470161	-20.952374	9.554496
-83.246570	-28.808288	9.564493
-81.450631	-25.734935	9.574490
-79.782789	-21.261213	9.584487
-77.903534	-20.368936	9.594483
-75.847376	-27.222392	9.604480
-73.790654	-20.151889	9.614477
-72.084304	-29.680979	9.624474
-70.504102	-29.730939	9.634471
-68.546117	-28.840163	9.644467
-66.721441	-33.397319	9.654464
-64.755868	-27.957452	9.664461
-62.812646	-34.033442	9.674458
-60.943751	-29.348636	9.684455
-58.962700	-32.493962	9.694451
-57.317318	-26.701445	9.704448
-55.441120	-28.050658	9.714445
-53.104274	-25.013047	9.724442
-51.223545	-19.629100	9.734439
-49.708285	-19.123977	9.744435
-47.772137	-17.823930	9.754432
-46.063485	-22.957800	9.764429
-44.025504	-17.471043	9.774426
-42.105799	-23.053821	9.784423
-40.063093	-29.543541	9.794419
-38.519191	-29.260864	9.804416
-37.009917	-25.601776	9.814413
-34.814230	-30.447029	9.824410
-32.490974	-28.359289	9.834407
-30.910714	-28.996572	9.844403
-28.947146	-23.381097	9.854400
-27.025367	-25.629620	9.864397
-25.244220	-18.613004	9.874394
-23.407517	-26.964497	9.884391
-21.599797	-25.748149	9.894387
-19.671543	-29.046068	9.904384
-17.706043	-32.240985	9.914381
-16.000757	-29.219435	9.924378
-14.019936	-26.068158	9.934375
-12.152487	-32.864620	9.944371
-10.286147	-26.887850	9.954368
-8.511108	-33.604836	9.964365
-6.409760	-26.205093	9.974362
-4.937214	-20.375493	9.984359
-3.849224	14.195675	9.994355
-2.581691	61.705622	10.004352
-1.142221	128.772805	10.014349
0.000000	172.834328	10.019354
0.362687	213.530831	10.024359
0.991533	250.873545	10.029363
1.606734	281.907839	10.034368
1.932472	327.073139	10.039373
2.089633	350.414458	10.044378
2.262453	364.750828	10.049383
2.644064	380.465232	10.054387
3.157966	401.836960	10.059392
3.282035	425.022834	10.064397
3.399879	418.384230	10.069402
3.420946	423.434851	10.074407
3.458123	431.064291	10.079411
3.322938	447.137154	10.084416
3.740258	448.008866	10.089421
4.325097	466.182455	10.094426
4.138298	483.170310	10.099431
4.229590	471.373126	10.104435
4.355549	480.656797	10.109440
4.101683	485.170990	10.114445
4.183675	482.557611	10.119450
3.736442	495.444487	10.124455
4.125113	486.976018	10.129459
4.167928	484.837229	10.134464
4.205839	487.674363	10.139469
4.065379	492.108970	10.144474
3.908539	509.095231	10.149479
4.820393	507.779742	10.154483
4.541240	522.391779	10.159488
4.353947	510.684727	10.164493
4.964769	526.296500	10.169498
4.901471	531.589268	10.174503
4.874528	527.187692	10.179507
4.353509	519.376795	10.184512
4.544324	537.122901	10.189517
4.728234	533.435149	10.194522
4.702293	541.010061	10.199527
4.707222	552.110763	10.204531
4.870870	554.588819	10.209536
5.031096	553.662862	10.214541
4.986610	553.761436	10.219546
5.037944	550.982628	10.224551
5.104138	551.451470	10.229555
4.810883	557.985687	10.234560
4.845043	561.600852	10.239565
5.506126	574.670560	10.244570
5.474013	586.690231	10.249575
5.232821	584.267150	10.254579
5.254245	599.816897	10.259584
5.216992	598.769474	10.264589
5.434986	590.058515	10.269594
5.333481	600.488694	10.274599
5.574595	596.004920	10.279603
5.451185	601.592723	10.284608
5.360460	601.823249	10.289613
5.713831	603.909938	10.294618
5.492459	602.123922	10.299623
5.801570	605.025053	10.304627
5.622305	624.088675	10.309632
5.942491	631.065966	10.314637
6.286931	644.231971	10.319642
6.139724	641.711890	10.324647
5.971191	626.111482	10.329651
5.710226	630.336698	10.334656
5.989320	650.503631	10.339661
6.317690	645.081846	10.344666
6.248481	647.060904	10.349671
6.354350	652.435541	10.354675
6.155729	652.981316	10.359680
6.410481	659.732519	10.364685
6.104666	657.076886	10.369690
6.129717	667.132119	10.374695
6.309370	664.991978	10.379699
6.407734	664.563152	10.384704
6.548060	668.030526	10.389709
6.832004	663.675515	10.394714
6.597911	670.119923	10.399719
6.687187	671.195357	10.404723
6.594039	677.547903	10.409728
6.382014	671.412798	10.414733
6.624133	672.769779	10.419738
6.679202	691.323035	10.424743
6.826424	706.423907	10.429747
7.198318	712.347485	10.434752
6.798387	714.888650	10.439757
7.212042	695.568366	10.444762
6.981848	710.825633	10.449767
7.065235	713.463172	10.454771
6.996049	711.725407	10.459776
7.006174	713.728090	10.464781
7.021983	713.250930	10.469786
6.818539	718.648119	10.474791
7.331805	723.834803	10.479795
7.301020	737.522782	10.484800
6.936861	752.109185	10.489805
7.798696	745.645076	10.494810
7.810220	755.341410	10.499815
7.696566	748.597654	10.504819
7.709033	742.144442	10.509824
7.396104	755.169396	10.514829
7.588320	748.717473	10.519834
7.279855	772.154239	10.524839
7.809335	751.550703	10.529843
7.484144	768.433233	10.534848
7.385485	768.414294	10.539853
7.790827	765.372402	10.544858
7.753109	773.616358	10.549863
7.878518	769.016945	10.554867
7.912230	799.074357	10.559872
8.207881	795.389216	10.564877
8.326981	802.802360	10.569882
8.122035	805.566329	10.574887
8.299263	797.289100	10.579891
8.506482	793.870375	10.584896
8.243287	813.734525	10.589901
8.317319	803.556190	10.594906
8.056397	804.028329	10.599911
8.340410	811.842526	10.604915
8.446693	804.325656	10.609920
8.410174	810.752805	10.614925
8.502385	818.422557	10.619930
8.496554	812.703933	10.624935
8.677205	815.188784	10.629939
8.948993	810.857745	10.634944
8.853059	820.203834	10.639949
8.781357	819.824206	10.644954
8.710392	820.780131	10.649959
8.712325	809.432161	10.654963
8.670182	821.925133	10.659968
8.848838	818.846847	10.664973
8.952774	834.516149	10.669978
8.875179	851.652596	10.674983
8.968504	853.955840	10.679987
9.388305	860.911047	10.684992
9.159280	857.216535	10.689997
9.424320	855.750297	10.695002
9.329772	864.222564	10.700007
9.186808	862.627435	10.705011
9.007032	868.963919	10.710016
9.243833	852.623683	10.715021
9.119934	866.309289	10.720026
9.131927	875.294425	10.725031
9.378014	869.420481	10.730035
9.397528	870.691561	10.735040
9.714861	885.686640	10.740045
9.834374	893.703737	10.745050
9.762271	895.156588	10.750055
9.998274	893.523089	10.755059
9.895513	903.397022	10.760064
9.720729	902.168087	10.765069
10.213120	897.289328	10.770074
9.857385	891.738445	10.775079
9.700006	893.581789	10.780083
9.572557	896.696113	10.785088
9.445965	909.554289	10.790093
10.149304	911.391240	10.795098
9.693239	908.183937	10.800103
10.014920	903.097438	10.805107
9.874271	922.530607	10.810112
10.296877	939.964269	10.815117
10.467489	936.808394	10.820122
10.527979	939.790249	10.825127
10.309873	953.899395	10.830131
10.450652	943.191497	10.835136
10.627015	942.363869	10.840141
10.515094	944.032811	10.845146
10.287342	949.446577	10.850151
10.793113	946.382323	10.855155
10.555985	945.145981	10.860160
10.552268	947.264444	10.865165
10.467295	937.546616	10.870170
10.434147	951.132672	10.875175
10.718797	949.403099	10.880179
10.665914	953.631489	10.885184
10.793817	958.753566	10.890189
11.005714	967.881918	10.895194
10.768100	983.331465	10.900199
10.882321	983.418921	10.905203
10.898090	979.322633	10.910208
10.870487	984.508947	10.915213
11.227749	975.814969	10.920218
11.061689	982.221855	10.925223
10.965223	983.782680	10.930227
11.163320	989.284659	10.935232
11.028351	989.069660	10.940237
11.199485	1008.434291	10.945242
11.039256	1025.634586	10.950247
11.492162	1021.701956	10.955251
11.476312	1022.573409	10.960256
11.507524	1029.431402	10.965261
11.574354	1030.168243	10.970266
11.576237	1029.936146	10.975271
11.592557	1020.098027	10.980275
11.588460	1024.019033	10.985280
11.625415	1030.762570	10.990285
11.758970	1019.961150	10.995290
11.782180	1043.850081	11.000295
11.965271	1048.780460	11.005299
11.872940	1048.982863	11.010304
11.874517	1063.935448	11.015309
12.409255	1057.477644	11.020314
11.864859	1061.727689	11.025319
12.181534	1059.325937	11.030323
12.058893	1062.513647	11.035328
11.997231	1066.547926	11.040333
12.330088	1061.711905	11.045338
12.373521	1067.229120	11.050343
12.438003	1061.710498	11.055347
12.417203	1062.721517	11.060352
12.323731	1058.518050	11.065357
12.758913	1048.321366	11.070362
12.604295	1060.698440	11.075367
12.186925	1063.871656	11.080371
12.057840	1074.368076	11.085376
12.642181	1090.902483	11.090381
12.869945	1091.944822	11.095386
12.859337	1103.277085	11.100391
13.236681	1093.609996	11.105395
13.031708	1103.763722	11.110400
12.842042	1111.581090	11.115405
13.161063	1099.494758	11.120410
12.971362	1100.002855	11.125415
13.108054	1099.172083	11.130419
13.263107	1106.101826	11.135424
13.059604	1105.438855	11.140429
13.352386	1098.757847	11.145434
12.774598	1111.882133	11.150439
13.161984	1100.496112	11.155443
13.200488	1096.304701	11.160448
12.931324	1108.021987	11.165453
13.252965	1101.781080	11.170458
12.911261	1117.898662	11.175463
13.259785	1113.865960	11.180467
13.237219	1108.965185	11.185472
13.298801	1123.788411	11.190477
13.470347	1135.173649	11.195482
13.220361	1148.504310	11.200487
13.588290	1137.154480	11.205491
13.672477	1134.904916	11.210496
13.488442	1144.003487	11.215501
13.589726	1134.252666	11.220506
13.664841	1148.203267	11.225511
13.981208	1152.409092	11.230515
13.914387	1167.940405	11.235520
14.217891	1162.192808	11.240525
14.228209	1161.448422	11.245530
14.134881	1164.385469	11.250535
14.432918	1154.653717	11.255539
14.374171	1149.362877	11.260544
13.781087	1150.077241	11.265549
14.542044	1151.758377	11.270554
14.065566	1170.868543	11.275559
14.022831	1165.854269	11.280563
14.621074	1168.699939	11.285568
14.231864	1163.548535	11.290573
14.863378	1163.834189	11.295578
14.380991	1168.583739	11.300583
14.862138	1172.181383	11.305587
14.963354	1164.988416	11.310592
14.836249	1176.162695	11.315597
15.062638	1173.158725	11.320602
15.059827	1168.997537	11.325607
14.981114	1159.604997	11.330611
14.722527	1154.065326	11.335616
14.672012	1165.746208	11.340621
14.913242	1169.700666	11.345626
14.683214	1184.685584	11.350631
14.640240	1177.580265	11.355635
15.037687	1177.948985	11.360640
15.030731	1176.385746	11.365645
15.109886	1169.494345	11.370650
14.824882	1181.895472	11.375655
15.125384	1174.565058	11.380659
15.280161	1185.596613	11.385664
15.104700	1174.339730	11.390669
15.678637	1187.029650	11.395674
15.228209	1177.704269	11.400679
15.335596	1199.195633	11.405683
15.605191	1204.342508	11.410688
15.498049	1204.898944	11.415693
15.605310	1204.497069	11.420698
15.368568	1212.476544	11.425703
15.720913	1203.892028	11.430707
15.451232	1212.704674	11.435712
15.482111	1217.613655	11.440717
15.537966	1207.991458	11.445722
15.184166	1217.889874	11.450727
15.321157	1222.744085	11.455731
15.985069	1227.932158	11.460736
15.996416	1251.394382	11.465741
16.123098	1233.836499	11.470746
15.784113	1250.729672	11.475751
16.280721	1238.271118	11.480755
15.924969	1244.989077	11.485760
16.095899	1247.497631	11.490765
16.092209	1234.852363	11.495770
15.808799	1243.607292	11.500775
15.921246	1242.709415	11.505779
16.153106	1257.185490	11.510784
16.220452	1264.506198	11.515789
16.540967	1272.251743	11.520794
16.544923	1270.106420	11.525799
16.715752	1270.314163	11.530803
16.931968	1264.326552	11.535808
16.541121	1275.140839	11.540813
17.014878	1267.863172	11.545818
16.719120	1269.561472	11.550823
16.963471	1272.474646	11.555827
17.214144	1254.766071	11.560832
17.288738	1263.375601	11.565837
17.126562	1250.389734	11.570842
17.004839	1241.136468	11.575847
16.963026	1228.588751	11.580851
16.788024	1247.305572	11.585856
17.035553	1258.899568	11.590861
17.600670	1267.788841	11.595866
16.749780	1256.677469	11.600871
16.925118	1259.869737	11.605875
17.047440	1267.322030	11.610880
16.851804	1269.453803	11.615885
17.326167	1272.301906	11.620890
17.175048	1281.822677	11.625895
17.378033	1277.480398	11.630899
17.371365	1275.481852	11.635904
17.286500	1277.860894	11.640909
17.510081	1265.624063	11.645914
17.713195	1278.262818	11.650919
17.525828	1289.948280	11.655923
17.958115	1296.433340	11.660928
18.038647	1287.456876	11.665933
18.023073	1280.548992	11.670938
17.506862	1286.226515	11.675943
17.892749	1275.905068	11.680947
17.867685	1282.149245	11.685952
17.701937	1300.337942	11.690957
18.100918	1308.211345	11.695962
18.132780	1306.725481	11.700967
18.296750	1306.287751	11.705971
18.364328	1300.989323	11.710976
18.535644	1298.009882	11.715981
18.421948	1290.089442	11.720986
18.145599	1290.592441	11.725991
18.349354	1281.403934	11.730995
18.397653	1291.820178	11.736000
18.514529	1296.485229	11.741005
18.511884	1282.256450	11.746010
18.269789	1289.751107	11.751015
18.366191	1305.805329	11.756019
18.725961	1309.294631	11.761024
18.931639	1300.873803	11.766029
18.715935	1307.641996	11.771034
19.082534	1310.600337	11.776039
19.155872	1284.306458	11.781043
18.976020	1272.332667	11.786048
18.648935	1263.824940	11.791053
18.995966	1264.531295	11.796058
18.811526	1259.509627	11.801063
18.887140	1261.665947	11.806067
19.062322	1274.914720	11.811072
18.979526	1295.015689	11.816077
19.197943	1297.967699	11.821082
18.735267	1302.274166	11.826087
19.066172	1300.422054	11.831091
19.094293	1309.512122	11.836096
18.849547	1311.207022	11.841101
18.973780	1307.178500	11.846106
18.872878	1300.728928	11.851111
19.317407	1311.984032	11.856115
19.506032	1326.949634	11.861120
19.247415	1323.895252	11.866125
19.663383	1331.803807	11.871130
19.663118	1347.095244	11.876135
19.518431	1340.732276	11.881139
19.817757	1327.838318	11.886144
19.736826	1343.886961	11.891149
19.887585	1336.477055	11.896154
19.512828	1335.168009	11.901159
19.846645	1327.679235	11.906163
20.058052	1340.028132	11.911168
19.933786	1334.624668	11.916173
20.076648	1331.816920	11.921178
19.684654	1334.539855	11.926183
19.601017	1342.418497	11.931187
19.937014	1331.627925	11.936192
19.575376	1347.249820	11.941197
20.007228	1345.816855	11.946202
20.018456	1369.459067	11.951207
20.237685	1365.049513	11.956211
20.632654	1375.333253	11.961216
20.761838	1369.941394	11.966221
20.989046	1339.947667	11.971226
20.754891	1352.581321	11.976231
20.676556	1342.611419	11.981235
20.793034	1331.931555	11.986240
20.755223	1335.403847	11.991245
20.754700	1335.135858	11.996250
20.751693	1325.136607	12.001255
20.951057	1332.422101	12.006259
20.733307	1333.696369	12.011264
20.444232	1337.524136	12.016269
20.783443	1323.094132	12.021274
20.603738	1329.298336	12.026279
20.591368	1335.939492	12.031283
20.841865	1351.635653	12.036288
20.994151	1356.637285	12.041293
21.194506	1351.380743	12.046298
20.748063	1351.937681	12.051303
20.734010	1334.136398	12.056307
21.070631	1342.034747	12.061312
20.863256	1333.724723	12.066317
20.907675	1331.617094	12.071322
20.988555	1340.520566	12.076327
20.754671	1335.566683	12.081331
20.840690	1339.137501	12.086336
21.025654	1328.980530	12.091341
20.836939	1340.248342	12.096346
20.755145	1336.744696	12.101351
20.644456	1341.440537	12.106355
20.779663	1349.007516	12.111360
21.176056	1360.817555	12.116365
21.422097	1342.778441	12.121370
20.693078	1345.736486	12.126375
20.879541	1340.669037	12.131379
20.980014	1341.970614	12.136384
20.937505	1340.290810	12.141389
21.207452	1332.654521	12.146394
20.773788	1340.842097	12.151399
21.038223	1326.832459	12.156403
21.056525	1336.077078	12.161408
20.573830	1352.301776	12.166413
21.100825	1345.360943	12.171418
21.016390	1347.085472	12.176423
20.914067	1341.560231	12.181427
20.893204	1337.755910	12.186432
20.834817	1352.772764	12.191437
21.024318	1345.557742	12.196442
21.213818	1350.613363	12.201447
21.173365	1347.044772	12.206451
21.767870	1342.108580	12.211456
21.332757	1336.539432	12.216461
21.368967	1324.786611	12.221466
20.951486	1315.815440	12.226471
21.067172	1313.698024	12.231475
21.224406	1318.563232	12.236480
21.034611	1325.332032	12.241485
21.144145	1305.542190	12.246490
20.927063	1313.166915	12.251495
20.996092	1282.360361	12.256499
20.697673	1288.075690	12.261504
20.569960	1290.346448	12.266509
21.028466	1301.291801	12.271514
21.167128	1310.985576	12.276519
20.923313	1297.766675	12.281523
20.944409	1278.238564	12.286528
20.402754	1283.189996	12.291533
21.070128	1290.533292	12.296538
20.746524	1304.960810	12.301543
21.034078	1308.680832	12.306547
21.042972	1289.238233	12.311552
20.922595	1286.527673	12.316557
21.188776	1285.824476	12.321562
20.944581	1285.450269	12.326567
21.089192	1294.718872	12.331571
20.812113	1286.504362	12.336576
20.686843	1289.981131	12.341581
21.061813	1285.173014	12.346586
20.701294	1292.959381	12.351591
20.582067	1289.734537	12.356595
20.793388	1288.718383	12.361600
20.812169	1292.329876	12.366605
20.664862	1286.255151	12.371610
20.837930	1279.397607	12.376615
20.829485	1286.225776	12.381619
20.885775	1291.898726	12.386624
20.727173	1295.574782	12.391629
21.293963	1282.322808	12.396634
20.741272	1286.815519	12.401639
20.909380	1296.063029	12.406643
20.925824	1294.626935	12.411648
20.747583	1308.428860	12.416653
20.790297	1289.274189	12.421658
21.033061	1288.467491	12.426663
20.984558	1290.962165	12.431667
21.000665	1288.810170	12.436672
20.727877	1292.498129	12.441677
21.311439	1295.551178	12.446682
20.810104	1294.620301	12.451687
20.755747	1292.487429	12.456691
21.171563	1295.726508	12.461696
20.771120	1300.202826	12.466701
21.255921	1284.803442	12.471706
20.985755	1286.972337	12.476711
21.183446	1289.432475	12.481715
20.777943	1289.306351	12.486720
21.062961	1296.868332	12.491725
21.109878	1289.750198	12.496730
21.143054	1289.954664	12.501735
21.083054	1287.784846	12.506739
21.215812	1288.019162	12.511744
20.427680	1273.802127	12.516749
20.856622	1278.008959	12.521754
21.111403	1287.215831	12.526759
21.110735	1283.486364	12.531763
20.834433	1272.868400	12.536768
20.684940	1262.742741	12.541773
20.938441	1264.072732	12.546778
20.718258	1271.488190	12.551783
20.579693	1265.662821	12.556787
20.867412	1271.585864	12.561792
21.256438	1285.969092	12.566797
21.047365	1277.776857	12.571802
21.055659	1275.192438	12.576807
20.909651	1257.332656	12.581811
20.920536	1260.639465	12.586816
20.668179	1259.137434	12.591821
21.080856	1254.861068	12.596826
20.978395	1272.856707	12.601831
20.966326	1271.679059	12.606835
20.903720	1267.322371	12.611840
20.962633	1265.338599	12.616845
20.952504	1267.357204	12.621850
20.800646	1266.949346	12.626855
21.097099	1264.547633	12.631859
20.892985	1259.883925	12.636864
20.656849	1273.067408	12.641869
20.942917	1267.995926	12.646874
20.892569	1268.377721	12.651879
21.038434	1280.653439	12.656883
20.907320	1273.353968	12.661888
20.760375	1272.864899	12.666893
20.864599	1272.163879	12.671898
20.700570	1281.609437	12.676903
21.038885	1275.898822	12.681907
21.114393	1274.536890	12.686912
20.603454	1270.981854	12.691917
20.961192	1265.288646	12.696922
20.752593	1268.649387	12.701927
20.834641	1273.327870	12.706931
20.790499	1271.669624	12.711936
20.783252	1274.228679	12.716941
20.831665	1264.842603	12.721946
20.939856	1272.853832	12.726951
20.714962	1277.590733	12.731955
20.800925	1273.885300	12.736960
20.553926	1281.442238	12.741965
20.685200	1270.428102	12.746970
20.585092	1270.136572	12.751975
20.697038	1293.314731	12.756979
20.663608	1298.737059	12.761984
20.742958	1303.824424	12.766989
21.070097	1302.778758	12.771994
20.820082	1308.770234	12.776999
21.078361	1312.676281	12.782003
20.962224	1302.315032	12.787008
20.705539	1295.101811	12.792013
20.993491	1298.217777	12.797018
20.812360	1299.221267	12.802023
20.591484	1284.374416	12.807027
20.736692	1306.233655	12.812032
20.968973	1316.404524	12.817037
21.252235	1306.996735	12.822042
20.778127	1301.620694	12.827047
20.848536	1306.758373	12.832051
20.963201	1297.598259	12.837056
20.574583	1292.747919	12.842061
20.918776	1296.534600	12.847066
20.972770	1316.728903	12.852071
20.861840	1315.655331	12.857075
20.923384	1304.778450	12.862080
20.758026	1307.648165	12.867085
21.018380	1305.957120	12.872090
20.366457	1306.209352	12.877095
20.938313	1313.500083	12.882099
20.755168	1312.647770	12.887104
20.567909	1316.801501	12.892109
20.541985	1305.943301	12.897114
20.592541	1321.528600	12.902119
20.479893	1318.151309	12.907123
20.915418	1319.745596	12.912128
20.783483	1324.732622	12.917133
20.919813	1306.059752	12.922138
20.333971	1325.203331	12.927143
20.605372	1319.041311	12.932147
21.313250	1309.187318	12.937152
20.984250	1314.612636	12.942157
21.111843	1320.219030	12.947162
21.040052	1316.283273	12.952167
20.896214	1318.447794	12.957171
20.975076	1324.273279	12.962176
21.063923	1324.785844	12.967181
21.233774	1319.124158	12.972186
21.078039	1327.043466	12.977191
21.175542	1324.257147	12.982195
21.332042	1322.874409	12.987200
20.566013	1316.881005	12.992205
20.955359	1307.467335	12.997210
20.982990	1328.342390	13.002215
21.064804	1303.930059	13.007219
20.970600	1300.825804	13.012224
20.923503	1299.964409	13.017229
21.237566	1281.922406	13.022234
20.919236	1289.586922	13.027239
20.767034	1294.607133	13.032243
20.867026	1285.596027	13.037248
20.837050	1290.691362	13.042253
20.876734	1287.169931	13.047258
20.742537	1294.358791	13.052263
20.801228	1295.164754	13.057267
20.747971	1286.458795	13.062272
20.539201	1302.347215	13.067277
20.810629	1298.599580	13.072282
20.527183	1301.259463	13.077287
20.663204	1316.181404	13.082291
20.859903	1321.371488	13.087296
20.636337	1333.911183	13.092301
20.939954	1316.974703	13.097306
21.233728	1330.901645	13.102311
21.143920	1329.723775	13.107315
21.053741	1310.706969	13.112320
20.628329	1308.846170	13.117325
21.386072	1301.961597	13.122330
20.909493	1302.783544	13.127335
21.065612	1304.430278	13.132339
21.145645	1301.121610	13.137344
20.934860	1297.977600	13.142349
21.139856	1293.049930	13.147354
20.811825	1290.873973	13.152359
20.669545	1301.719600	13.157363
20.874077	1312.218177	13.162368
20.607204	1304.490898	13.167373
21.186966	1292.441670	13.172378
21.008509	1295.527943	13.177383
20.731679	1300.432412	13.182387
21.081426	1293.351134	13.187392
20.970331	1304.797356	13.192397
20.907461	1299.614354	13.197402
20.842673	1310.832415	13.202407
21.097981	1298.382332	13.207411
21.017437	1299.120614	13.212416
20.838289	1300.798741	13.217421
21.225001	1289.242366	13.222426
21.089088	1296.575007	13.227431
21.030598	1297.024335	13.232435
21.018684	1301.747777	13.237440
20.939450	1287.004492	13.242445
21.123753	1280.302854	13.247450
20.774699	1270.716810	13.252455
20.647517	1266.048715	13.257459
20.947710	1265.341671	13.262464
20.594726	1276.435356	13.267469
21.142643	1274.602254	13.272474
21.034457	1279.186498	13.277479
20.749618	1269.233812	13.282483
21.038660	1267.017789	13.287488
20.788911	1265.244099	13.292493
20.949825	1260.853340	13.297498
20.879732	1278.883249	13.302503
20.816872	1270.003785	13.307507
21.142414	1260.335386	13.312512
20.695865	1274.550665	13.317517
21.004275	1260.166637	13.322522
20.756901	1270.745144	13.327527
20.703285	1273.625416	13.332531
20.737122	1269.147687	13.337536
20.642426	1272.923934	13.342541
20.720033	1275.743853	13.347546
21.124603	1291.113381	13.352551
21.048187	1285.595068	13.357555
21.000892	1283.806433	13.362560
20.787025	1274.290290	13.367565
20.962285	1280.062535	13.372570
20.812201	1262.244400	13.377575
20.662017	1270.342568	13.382579
20.993905	1267.009509	13.387584
20.744907	1281.275290	13.392589
21.119549	1262.239606	13.397594
20.864576	1275.743071	13.402599
20.797499	1273.254254	13.407603
20.917413	1262.275052	13.412608
20.784796	1273.204274	13.417613
21.041068	1270.335871	13.422618
21.087757	1283.193550	13.427623
20.944205	1280.016743	13.432627
21.002003	1274.814505	13.437632
20.974137	1280.395214	13.442637
20.956933	1275.955586	13.447642
21.013982	1275.569603	13.452647
20.956507	1270.800501	13.457651
21.157213	1277.281487	13.462656
20.478698	1287.151312	13.467661
20.738560	1273.935681	13.472666
20.879219	1278.149068	13.477671
20.662164	1274.690665	13.482675
21.026904	1275.564512	13.487680
20.848857	1279.256281	13.492685
21.297261	1272.381635	13.497690
21.088274	1278.782881	13.502695
21.171352	1289.262964	13.507699
21.589005	1272.543320	13.512704
21.199814	1272.237971	13.517709
21.130688	1248.315020	13.522714
20.928396	1254.387173	13.527719
20.867625	1253.384456	13.532723
21.067798	1244.721682	13.537728
20.869515	1254.535392	13.542733
21.071124	1238.790130	13.547738
20.893639	1251.445410	13.552743
20.752300	1244.915577	13.557747
20.986697	1245.745555	13.562752
20.828357	1242.889667	13.567757
20.892384	1252.789276	13.572762
20.856889	1242.935615	13.577767
20.993711	1246.829475	13.582771
20.645519	1253.115714	13.587776
20.875690	1245.624590	13.592781
20.949943	1247.391609	13.597786
21.106770	1249.192768	13.602791
20.726603	1251.167885	13.607795
21.171411	1238.698669	13.612800
20.843378	1248.794850	13.617805
20.733230	1260.032722	13.622810
20.914912	1254.848580	13.627815
20.677025	1262.094964	13.632819
20.730360	1256.294188	13.637824
20.761637	1256.921590	13.642829
20.641082	1253.255408	13.647834
20.669779	1252.884987	13.652839
20.661297	1260.995244	13.657843
20.878678	1256.932956	13.662848
20.770204	1258.273370	13.667853
20.827327	1252.867815	13.672858
20.653988	1255.562170	13.677863
20.743113	1251.971358	13.682867
20.919473	1260.985712	13.687872
20.473671	1271.616369	13.692877
21.022741	1276.624077	13.697882
20.839567	1284.402654	13.702887
20.803852	1284.698535	13.707891
20.914712	1291.119738	13.712896
20.726749	1288.978213	13.717901
20.699055	1288.164188	13.722906
20.952517	1288.325635	13.727911
20.791779	1281.742109	13.732915
20.906925	1281.668566	13.737920
20.544132	1292.902603	13.742925
20.709447	1285.522730	13.747930
20.998989	1287.457273	13.752935
21.053387	1297.222826	13.757939
21.196444	1289.215704	13.762944
21.092417	1287.497619	13.767949
21.220264	1275.544137	13.772954
20.824793	1272.486361	13.777959
20.939990	1263.748817	13.782963
20.826534	1260.368514	13.787968
20.735052	1250.686207	13.792973
20.870364	1255.640048	13.797978
20.680282	1255.481143	13.802983
20.588557	1267.025173	13.807987
20.849918	1274.849543	13.812992
20.755055	1286.241120	13.817997
20.974369	1279.250040	13.823002
20.832901	1294.999982	13.828007
21.166008	1284.912457	13.833011
20.994391	1282.542816	13.838016
20.913905	1294.234889	13.843021
20.772229	1268.584050	13.848026
20.934651	1264.361787	13.853031
20.817459	1270.322602	13.858035
20.849388	1266.282004	13.863040
20.740713	1274.061310	13.868045
20.802096	1281.832421	13.873050
20.580113	1293.201700	13.878055
21.028775	1288.388137	13.883059
20.914323	1287.744071	13.888064
20.794607	1293.848804	13.893069
21.059570	1294.989308	13.898074
21.014782	1295.535801	13.903079
20.792841	1279.848586	13.908083
20.925424	1275.440263	13.913088
20.622306	1272.325179	13.918093
20.723387	1272.706477	13.923098
20.937922	1277.863738	13.928103
20.967857	1292.794689	13.933107
21.334618	1278.338257	13.938112
20.726635	1279.494983	13.943117
20.929326	1267.017048	13.948122
20.900391	1254.587105	13.953127
20.800394	1272.530311	13.958131
21.010949	1270.221146	13.963136
20.680652	1270.251766	13.968141
20.731573	1261.973917	13.973146
20.913550	1272.293132	13.978151
20.798653	1287.045322	13.983155
21.173886	1286.745789	13.988160
20.428912	1270.938571	13.993165
20.999602	1273.861201	13.998170
21.195319	1292.807544	14.003175
20.994370	1277.214757	14.008179
21.027767	1266.041188	14.013184
20.599010	1266.797158	14.018189
21.107422	1259.519000	14.023207
20.938715	1270.544123	14.028224
20.698933	1269.325581	14.033242
21.300865	1260.639613	14.038259
20.655299	1268.464297	14.043277
20.993609	1270.035234	14.048295
20.969494	1270.028087	14.053312
20.681978	1275.049264	14.058330
20.642500	1277.512557	14.063347
20.711661	1292.822280	14.068365
20.930681	1298.910945	14.073383
20.820058	1297.803931	14.078400
20.933640	1313.119175	14.083418
21.005058	1305.428545	14.088435
21.073269	1314.836649	14.093453
21.296771	1300.671001	14.098471
21.309225	1312.563855	14.103488
21.251901	1310.249734	14.108506
21.400143	1306.092334	14.113523
21.030500	1303.376582	14.118541
21.357636	1304.746392	14.123559
21.232094	1304.215892	14.128576
21.312578	1309.713198	14.133594
21.471283	1312.954970	14.138611
21.444276	1318.552791	14.143629
21.182281	1302.037475	14.148647
21.332912	1313.840655	14.153664
21.128553	1301.783393	14.158682
21.061659	1312.745120	14.163699
21.056978	1306.542076	14.168717
21.543639	1308.521924	14.173735
21.649119	1301.846724	14.178752
21.244258	1298.642677	14.183770
21.345450	1299.688312	14.188787
21.332233	1307.643388	14.193805
21.514672	1298.178044	14.198823
21.533578	1306.414278	14.203840
21.388095	1307.949126	14.208858
21.393776	1311.746969	14.213875
21.200402	1307.521362	14.218893
21.217406	1311.296950	14.223911
21.305314	1317.784048	14.228928
21.225678	1337.037403	14.233946
21.856945	1335.307134	14.238963
21.615454	1340.347733	14.243981
21.845316	1348.366306	14.248999
21.874048	1333.147909	14.254016
21.692223	1338.347300	14.259034
21.923088	1336.279784	14.264051
21.695230	1352.483203	14.269069
21.814471	1339.644437	14.274087
21.823234	1341.220752	14.279104
21.591563	1352.186767	14.284122
21.727556	1338.440868	14.289139
21.560270	1346.087067	14.294157
21.456460	1337.106213	14.299175
21.376137	1348.833002	14.304192
21.506627	1347.096089	14.309210
21.634991	1347.358770	14.314227
21.949203	1365.865101	14.319245
22.052589	1372.153133	14.324263
22.392465	1373.805627	14.329280
21.684879	1351.988022	14.334298
21.962941	1343.271865	14.339315
21.717956	1353.606095	14.344333
22.201888	1356.051987	14.349351
22.000956	1365.724840	14.354368
21.721096	1364.037643	14.359386
22.092204	1364.871924	14.364403
21.699167	1370.674431	14.369421
22.104270	1381.192066	14.374439
22.298619	1370.814806	14.379456
22.148246	1384.653511	14.384474
22.389120	1382.109352	14.389491
21.984359	1379.973325	14.394509
22.327615	1378.951213	14.399527
22.600155	1382.277088	14.404544
22.158779	1380.546438	14.409562
22.380176	1372.020981	14.414579
22.134786	1380.520413	14.419597
22.193984	1376.660332	14.424615
22.322458	1381.651377	14.429632
21.874883	1379.525324	14.434650
22.053498	1381.972726	14.439667
22.034310	1381.842101	14.444685
22.004927	1391.039311	14.449703
22.451825	1400.646615	14.454720
22.609687	1414.959205	14.459738
22.781406	1411.947883	14.464755
22.762468	1412.660337	14.469773
22.362260	1391.388237	14.474791
22.778555	1381.278370	14.479808
22.633346	1387.293034	14.484826
22.619111	1380.880703	14.489843
22.826861	1385.690796	14.494861
22.595874	1382.156986	14.499879
22.599278	1380.838303	14.504896
22.784611	1385.346813	14.509914
22.851900	1376.571447	14.514931
22.449655	1386.531245	14.519949
22.550519	1384.404234	14.524967
22.797304	1383.918165	14.529984
22.776770	1387.050118	14.535002
22.691608	1384.079772	14.540019
22.806884	1379.696381	14.545037
22.509450	1380.157531	14.550055
23.106656	1401.896866	14.555072
22.975130	1407.983287	14.560090
22.524151	1384.086119	14.565107
22.560942	1400.714558	14.570125
22.621157	1416.120217	14.575143
22.927550	1401.195656	14.580160
23.194025	1401.474062	14.585178
23.306335	1407.705632	14.590195
23.388422	1404.656698	14.595213
23.143858	1399.662174	14.600231
23.267725	1382.264128	14.605248
23.000026	1390.294443	14.610266
22.870377	1380.075027	14.615283
22.880526	1379.551197	14.620301
23.146559	1401.304026	14.625319
23.287901	1411.276241	14.630336
22.806069	1405.976647	14.635354
23.142709	1403.967754	14.640371
23.394686	1415.199590	14.645389
23.122263	1407.134321	14.650407
22.923807	1410.604535	14.655424
23.024863	1419.200527	14.660442
23.501961	1401.414220	14.665459
23.640113	1412.549380	14.670477
23.277736	1411.051511	14.675495
23.521277	1408.140417	14.680512
23.395090	1406.136130	14.685530
23.402101	1409.144148	14.690547
23.565864	1407.173838	14.695565
23.501518	1399.586608	14.700583
23.419774	1387.764542	14.705600
23.267408	1388.710628	14.710618
23.518638	1401.073545	14.715635
23.218061	1414.861519	14.720653
23.158343	1411.276791	14.725671
23.512160	1402.825362	14.730688
23.684759	1408.273409	14.735706
23.547066	1404.120688	14.740723
23.516656	1405.081929	14.745741
23.490676	1414.017496	14.750759
23.631365	1407.846278	14.755776
23.762103	1417.977488	14.760794
23.573302	1415.383878	14.765811
23.666035	1404.771910	14.770829
23.340728	1418.090363	14.775847
24.006535	1409.324909	14.780864
23.565020	1409.020974	14.785882
23.601847	1423.148388	14.790899
23.878464	1400.719145	14.795917
23.478279	1416.119584	14.800935
23.712488	1410.215014	14.805952
23.710958	1412.700592	14.810970
23.732429	1413.379860	14.815987
24.056391	1408.555774	14.821005
23.875863	1415.455381	14.826023
23.950664	1408.761430	14.831040
23.895853	1418.546290	14.836058
23.799808	1411.258257	14.841075
23.983844	1418.958570	14.846093
24.252494	1430.631340	14.851111
23.925839	1433.750780	14.856128
24.069663	1432.620477	14.861146
24.010557	1439.123212	14.866163
23.936388	1443.970424	14.871181
23.990216	1442.129325	14.876199
24.369028	1437.420747	14.881216
24.234550	1440.633805	14.886234
24.300318	1441.507352	14.891251
24.269048	1435.204677	14.896269
23.992878	1438.934251	14.901287
24.628968	1427.469561	14.906304
24.617383	1434.175495	14.911322
24.541000	1409.334522	14.916339
24.206974	1402.815886	14.921357
24.211548	1398.500481	14.926375
24.321523	1400.928948	14.931392
24.428493	1404.237192	14.936410
24.469340	1400.035548	14.941427
24.594803	1407.144317	14.946445
24.486277	1400.408825	14.951463
24.723598	1403.254271	14.956480
24.297430	1405.395451	14.961498
24.198417	1407.498610	14.966515
24.693261	1398.321567	14.971533
24.244620	1414.929920	14.976551
24.578034	1412.919968	14.981568
24.307932	1419.692295	14.986586
24.494149	1420.417645	14.991603
24.702927	1432.243107	14.996621
24.417957	1427.275467	15.001639
24.618151	1428.852721	15.006656
24.617564	1436.028798	15.011674
24.732847	1420.623476	15.016691
24.652046	1419.609221	15.021709
24.619761	1436.874767	15.026727
24.723504	1431.610754	15.031744
24.378877	1444.825350	15.036762
24.322994	1432.981819	15.041779
24.802311	1431.420491	15.046797
24.628583	1429.241316	15.051815
24.696006	1428.831042	15.056832
25.051441	1446.081951	15.061850
24.855443	1443.376229	15.066867
25.038210	1453.002101	15.071885
25.056815	1461.694637	15.076903
24.990716	1442.075868	15.081920
24.954490	1450.626136	15.086938
25.190166	1455.965042	15.091955
25.054957	1446.822391	15.096973
24.863524	1442.096224	15.101991
25.243544	1453.917988	15.107008
25.272935	1467.074524	15.112026
25.173882	1459.445607	15.117043
25.146968	1447.767327	15.122061
25.156072	1462.289303	15.127079
25.452582	1463.572779	15.132096
25.408945	1450.306872	15.137114
25.162708	1435.604119	15.142131
25.271806	1429.570061	15.147149
25.187835	1434.582424	15.152167
25.325629	1429.128941	15.157184
25.233727	1433.919204	15.162202
25.295680	1447.916797	15.167219
25.666356	1445.749890	15.172237
25.611690	1443.076682	15.177255
25.287887	1444.317522	15.182272
25.509806	1431.338032	15.187290
25.251243	1436.533967	15.192307
25.448764	1443.387449	15.197325
25.437073	1461.269497	15.202343
25.885556	1462.374582	15.207360
25.523825	1454.993624	15.212378
25.409527	1449.658990	15.217395
25.976982	1452.856050	15.222413
25.553673	1451.882263	15.227431
25.549646	1452.032357	15.232448
25.986131	1455.407606	15.237466
25.723224	1441.482989	15.242483
25.798771	1431.211935	15.247501
25.311842	1443.411053	15.252519
25.794487	1453.947048	15.257536
26.066417	1465.551684	15.262554
25.754238	1449.177908	15.267571
25.834287	1452.891569	15.272589
25.627300	1460.715616	15.277607
25.487244	1469.930527	15.282624
25.672235	1463.950417	15.287642
25.735546	1458.755762	15.292659
26.157687	1458.164647	15.297677
26.153273	1463.795100	15.302695
25.844890	1461.253587	15.307712
26.072651	1463.900800	15.312730
25.989491	1465.235392	15.317747
26.258043	1446.466140	15.322765
26.015245	1463.265082	15.327783
26.349909	1455.695979	15.332800
26.293418	1465.577091	15.337818
26.221291	1461.210981	15.342835
26.233527	1459.972677	15.347853
26.048138	1476.680683	15.352871
26.564636	1468.972463	15.357888
26.446300	1456.292605	15.362906
26.012464	1462.699390	15.367923
26.229626	1469.169089	15.372941
26.312854	1452.154957	15.377959
26.047082	1459.705241	15.382976
26.212284	1467.798686	15.387994
25.976442	1460.595844	15.393011
26.098845	1455.209299	15.398029
25.946461	1467.193063	15.403047
26.123582	1468.242330	15.408064
26.597389	1479.935902	15.413082
26.259376	1488.016809	15.418099
26.603511	1485.681101	15.423117
26.644510	1483.697328	15.428135
26.861794	1491.206765	15.433152
26.748788	1480.240598	15.438170
26.394679	1488.232840	15.443187
26.697556	1482.322008	15.448205
26.861821	1490.612240	15.453223
26.898966	1473.663634	15.458240
26.607468	1463.891534	15.463258
26.457209	1459.193401	15.468275
26.539694	1477.573243	15.473293
26.931368	1479.088504	15.478311
26.695179	1482.201391	15.483328
26.886784	1487.006228	15.488346
26.719904	1480.566290	15.493363
26.748634	1482.485495	15.498381
27.018544	1487.361212	15.503399
27.008137	1492.283212	15.508416
27.235173	1480.122392	15.513434
27.004266	1499.706821	15.518451
26.916182	1477.905049	15.523469
27.204249	1490.763953	15.528487
27.004331	1481.752720	15.533504
26.960330	1481.276847	15.538522
26.738089	1491.404631	15.543539
27.270990	1480.876558	15.548557
27.086769	1475.007238	15.553575
26.964855	1493.449587	15.558592
27.223304	1488.766482	15.563610
27.006254	1487.355536	15.568627
27.340854	1490.902770	15.573645
27.461922	1477.750564	15.578663
27.173541	1481.612654	15.583680
27.250531	1483.843480	15.588698
27.169508	1473.372429	15.593715
27.338677	1481.576932	15.598733
26.920632	1486.082608	15.603751
26.716850	1487.823397	15.608768
26.903376	1483.191089	15.613786
26.963616	1505.903391	15.618803
27.286641	1506.182218	15.623821
27.436989	1515.980040	15.628839
27.322281	1521.053962	15.633856
27.566361	1514.889804	15.638874
27.671768	1514.453021	15.643891
27.473893	1507.240954	15.648909
27.404978	1510.245372	15.653927
27.392049	1512.868062	15.658944
27.533550	1503.025304	15.663962
27.406157	1510.185463	15.668979
27.814003	1514.126853	15.673997
27.701962	1515.159323	15.679015
27.595372	1522.621331	15.684032
27.800762	1527.348480	15.689050
27.814845	1545.341349	15.694067
27.984340	1529.799853	15.699085
27.829637	1525.712730	15.704103
27.906099	1525.071353	15.709120
28.263128	1522.787065	15.714138
28.223058	1513.906045	15.719155
28.382242	1504.197317	15.724173
27.984426	1502.525769	15.729191
28.145237	1505.037379	15.734208
28.159447	1515.495549	15.739226
28.010258	1510.396114	15.744243
27.900563	1502.979653	15.749261
28.165486	1511.743044	15.754279
27.760227	1506.664002	15.759296
28.405640	1503.130382	15.764314
28.085266	1510.181323	15.769331
28.367817	1504.475068	15.774349
28.312018	1508.411753	15.779367
28.165077	1497.458851	15.784384
28.542143	1499.084980	15.789402
27.931893	1508.420523	15.794419
27.909582	1504.452287	15.799437
28.385916	1507.431090	15.804455
28.171625	1512.852794	15.809472
28.232639	1518.483844	15.814490
28.428305	1529.378690	15.819507
28.324577	1542.293835	15.824525
28.599043	1528.033323	15.829543
28.585858	1535.939756	15.834560
28.575548	1540.713895	15.839578
28.443352	1533.120113	15.844595
28.806367	1531.558447	15.849613
28.513986	1539.029647	15.854631
28.295248	1530.383176	15.859648
28.871863	1536.855349	15.864666
28.680317	1532.289616	15.869683
28.577631	1537.506343	15.874701
28.841425	1530.849832	15.879719
28.839867	1526.033581	15.884736
28.846180	1534.993958	15.889754
28.768840	1537.299742	15.894771
29.044915	1531.618104	15.899789
28.966376	1525.948981	15.904807
28.709959	1529.106002	15.909824
29.065798	1534.748238	15.914842
28.416977	1537.654818	15.919859
28.723697	1528.375566	15.924877
28.751911	1516.391142	15.929895
28.786248	1535.518045	15.934912
28.931777	1533.036257	15.939930
28.638624	1530.662186	15.944947
29.220657	1535.046127	15.949965
29.367570	1540.260798	15.954983
29.040539	1540.259492	15.960000
29.092366	1531.661101	15.965018
29.082527	1541.841559	15.970035
29.249964	1546.554318	15.975053
29.554550	1544.182438	15.980071
29.122623	1544.010674	15.985088
29.411596	1542.040826	15.990106
29.364272	1530.686626	15.995123
29.171103	1526.132165	16.000141
29.482380	1542.995411	16.005159
29.429766	1548.224604	16.010176
29.402810	1552.518491	16.015194
29.533191	1561.975042	16.020211
29.174907	1559.147318	16.025229
29.526933	1547.314141	16.030247
29.727160	1565.988344	16.035264
29.805385	1555.334536	16.040282
29.728947	1550.152699	16.045299
29.815437	1533.097055	16.050317
29.588617	1523.229657	16.055335
29.376330	1524.386652	16.060352
29.605168	1526.635737	16.065370
29.609285	1545.043894	16.070387
29.580656	1545.751608	16.075405
29.732310	1545.007005	16.080423
29.560952	1556.359950	16.085440
29.426170	1549.011960	16.090458
29.520824	1564.868454	16.095475
29.696069	1557.752581	16.100493
29.782658	1551.560044	16.105511
29.481344	1557.874950	16.110528
29.845129	1558.825242	16.115546
29.695342	1574.211080	16.120563
29.944977	1590.233218	16.125581
30.139962	1585.030102	16.130599
30.355082	1587.260935	16.135616
30.515439	1585.569567	16.140634
30.434981	1565.671353	16.145651
30.054941	1554.190877	16.150669
30.234951	1548.423882	16.155687
29.912501	1559.835533	16.160704
30.319918	1557.096471	16.165722
30.413045	1560.581562	16.170739
30.010637	1560.961933	16.175757
30.453992	1568.636698	16.180775
30.519894	1582.775361	16.185792
30.275074	1569.580756	16.190810
30.339106	1562.073637	16.195827
30.379513	1580.572004	16.200845
30.684152	1574.451645	16.205863
30.628824	1570.329784	16.210880
30.464573	1559.897113	16.215898
30.445229	1564.896066	16.220915
30.650873	1566.798078	16.225933
30.964540	1569.030494	16.230951
30.571979	1561.832147	16.235968
30.728494	1543.933205	16.240986
30.446033	1555.948798	16.246003
30.473381	1544.054150	16.251021
30.896576	1557.797611	16.256039
30.360778	1574.251734	16.261056
30.874807	1565.414442	16.266074
31.206744	1577.907783	16.271091
30.879531	1564.712165	16.276109
31.003677	1556.692101	16.281127
30.689064	1545.212208	16.286144
30.756349	1560.926775	16.291162
30.791086	1562.313358	16.296179
30.915231	1576.324751	16.301197
31.377133	1563.247095	16.306215
30.874517	1582.049145	16.311232
30.805808	1573.723207	16.316250
30.786063	1573.210429	16.321267
31.115878	1582.797205	16.326285
31.248973	1571.009937	16.331303
30.978958	1580.077333	16.336320
30.919216	1581.419212	16.341338
31.151409	1579.812341	16.346355
31.156606	1579.449739	16.351373
31.182264	1573.786002	16.356391
30.752546	1580.050611	16.361408
31.144321	1569.192631	16.366426
31.215594	1578.864683	16.371443
31.366868	1590.936970	16.376461
31.549262	1588.903891	16.381479
31.133990	1601.426762	16.386496
31.736208	1597.275526	16.391514
31.695224	1599.569230	16.396531
31.267457	1607.768336	16.401549
31.448832	1593.816758	16.406567
31.565470	1609.411823	16.411584
31.532780	1607.705624	16.416602
31.697718	1596.627401	16.421619
31.564904	1602.204454	16.426637
31.775421	1599.172749	16.431655
31.965327	1607.789290	16.436672
31.655865	1601.965060	16.441690
31.841541	1601.078177	16.446707
31.511356	1607.070524	16.451725
31.950438	1604.092026	16.456743
32.130478	1594.611142	16.461760
32.005748	1603.850435	16.466778
31.718907	1599.244824	16.471795
32.088228	1596.710030	16.476813
32.013984	1600.442045	16.481831
32.107910	1601.493580	16.486848
31.932341	1609.430671	16.491866
32.090083	1599.465709	16.496883
31.906720	1606.973038	16.501901
31.916869	1600.330208	16.506919
32.103139	1605.889406	16.511936
32.048462	1603.227181	16.516954
32.219561	1603.621476	16.521971
32.077897	1603.024323	16.526989
32.195925	1609.171699	16.532007
32.100366	1603.583910	16.537024
32.095664	1609.651761	16.542042
32.301733	1596.227919	16.547059
31.986336	1601.841957	16.552077
32.454794	1606.984920	16.557095
32.623719	1616.794005	16.562112
32.379151	1614.228129	16.567130
32.240254	1611.884497	16.572147
32.377705	1613.081673	16.577165
32.659731	1613.080755	16.582183
32.610256	1620.895497	16.587200
32.652917	1618.845374	16.592218
33.040652	1610.445045	16.597235
32.238040	1621.140528	16.602253
32.913220	1612.928732	16.607271
32.731275	1620.734713	16.612288
32.780402	1607.663076	16.617306
33.056571	1610.418999	16.622323
32.946433	1611.009157	16.627341
33.032659	1606.594152	16.632359
32.842094	1622.563838	16.637376
33.062301	1610.973427	16.642394
33.016450	1594.939249	16.647411
32.655874	1616.375493	16.652429
32.771610	1614.980672	16.657447
32.916811	1604.435694	16.662464
32.698874	1611.698432	16.667482
33.285204	1613.272324	16.672499
33.012502	1606.822465	16.677517
32.934511	1606.438524	16.682535
32.781481	1618.164542	16.687552
33.027650	1611.298450	16.692570
33.210832	1604.403082	16.697587
33.241846	1612.656434	16.702605
33.137130	1609.928257	16.707623
33.430147	1600.619685	16.712640
33.004268	1613.295267	16.717658
33.103029	1620.485477	16.722675
33.251413	1650.402480	16.727693
33.527130	1640.382496	16.732711
33.684804	1640.313322	16.737728
33.406964	1647.766528	16.742746
33.661391	1639.406319	16.747763
33.499361	1651.305257	16.752781
33.588956	1647.905867	16.757799
33.924911	1646.977711	16.762816
33.663052	1651.022803	16.767834
34.050139	1644.832637	16.772851
33.696804	1646.726283	16.777869
34.131314	1642.120441	16.782887
34.005980	1640.032616	16.787904
33.852883	1629.827774	16.792922
33.872516	1608.815577	16.797939
33.638299	1617.488755	16.802957
33.855468	1627.637787	16.807975
33.983783	1642.680473	16.812992
34.037232	1641.418277	16.818010
33.960528	1650.099386	16.823027
33.637177	1653.072055	16.828045
33.608407	1646.649340	16.833063
33.816539	1644.789899	16.838080
33.732834	1646.942560	16.843098
33.967157	1631.102756	16.848115
33.656815	1642.514113	16.853133
33.861253	1656.042447	16.858151
33.881120	1667.722055	16.863168
34.012741	1666.738397	16.868186
34.367393	1672.977048	16.873203
34.217176	1671.873174	16.878221
34.721927	1663.653924	16.883239
34.535294	1663.870896	16.888256
34.202933	1665.805243	16.893274
34.604206	1661.379301	16.898291
34.530791	1668.748004	16.903309
34.492519	1670.602416	16.908327
34.955955	1671.130985	16.913344
34.732155	1676.255393	16.918362
34.995636	1665.196008	16.923379
34.610933	1669.328337	16.928397
34.907104	1662.589525	16.933415
35.100913	1670.195607	16.938432
34.707917	1644.053509	16.943450
35.262529	1633.726356	16.948467
34.686772	1636.037715	16.953485
34.335734	1628.327775	16.958503
34.746559	1637.580775	16.963520
34.744537	1653.051667	16.968538
35.140258	1663.159664	16.973555
34.838178	1659.600944	16.978573
34.923528	1660.188240	16.983591
34.985943	1663.701849	16.988608
34.734964	1664.721881	16.993626
35.386676	1649.249640	16.998643
35.391556	1659.158848	17.003661
35.264965	1658.972991	17.008679
35.170554	1660.210295	17.013696
35.235620	1667.051976	17.018714
35.342879	1658.921292	17.023731
35.362048	1669.210470	17.028749
35.502901	1660.361853	17.033767
35.465933	1657.792746	17.038784
35.067291	1656.116592	17.043802
35.562206	1654.236579	17.048819
35.470988	1662.875967	17.053837
35.342855	1656.459657	17.058855
35.115085	1659.031695	17.063872
35.178515	1654.887723	17.068890
35.061695	1649.688695	17.073907
34.858814	1665.956119	17.078925
35.163550	1682.960570	17.083943
35.582413	1684.933984	17.088960
35.453072	1697.482121	17.093978
36.029419	1684.826549	17.098995
35.709200	1691.613286	17.104013
35.967397	1700.801006	17.109031
36.029666	1687.401587	17.114048
36.184882	1684.943397	17.119066
36.029604	1692.727860	17.124083
35.937765	1686.395410	17.129101
35.795917	1687.294220	17.134119
36.230912	1685.636117	17.139136
36.039979	1685.021650	17.144154
36.363181	1697.305705	17.149171
36.219257	1686.662061	17.154189
36.161183	1694.040916	17.159207
36.072260	1685.738586	17.164224
35.869923	1696.283332	17.169242
36.478212	1682.966720	17.174259
36.000461	1688.545337	17.179277
35.889475	1689.192261	17.184295
36.103367	1682.282520	17.189312
36.009681	1702.004211	17.194330
36.021840	1682.525218	17.199347
36.050578	1691.779415	17.204365
35.993687	1701.037837	17.209383
36.345352	1713.034223	17.214400
36.458241	1702.494327	17.219418
36.522098	1706.273557	17.224435
36.657180	1701.275007	17.229453
36.777232	1717.824465	17.234471
36.926705	1704.485055	17.239488
36.717934	1712.537608	17.244506
36.842736	1715.770721	17.249523
36.897661	1704.931757	17.254541
36.795360	1712.003071	17.259559
36.996110	1704.200369	17.264576
36.794957	1708.053325	17.269594
37.064894	1701.905415	17.274611
36.936364	1705.878921	17.279629
36.716723	1707.145640	17.284647
36.962278	1699.996462	17.289664
36.846520	1709.097538	17.294682
36.676896	1703.121977	17.299699
36.544255	1712.101479	17.304717
36.561276	1709.734537	17.309735
36.713012	1726.013112	17.314752
37.240836	1731.807321	17.319770
37.274809	1739.250169	17.324787
37.369459	1731.867067	17.329805
37.418839	1736.773322	17.334823
37.574198	1734.101170	17.339840
37.348992	1741.349401	17.344858
37.478919	1740.490278	17.349875
38.007647	1740.023727	17.354893
37.751623	1713.184832	17.359911
37.809874	1700.978388	17.364928
37.851093	1696.219752	17.369946
37.745977	1695.314747	17.374963
37.580839	1700.900139	17.379981
37.465333	1702.274518	17.384999
37.694194	1689.823797	17.390016
37.521835	1705.125285	17.395034
37.394637	1699.737560	17.400051
37.412035	1701.694781	17.405069
37.444879	1725.536503	17.410087
37.622309	1727.364385	17.415104
37.608780	1741.910700	17.420122
38.020240	1723.289759	17.425139
38.112362	1733.202407	17.430157
38.019174	1739.927789	17.435175
38.113467	1729.414436	17.440192
37.750048	1736.779089	17.445210
37.869556	1729.676740	17.450227
37.508176	1738.848468	17.455245
37.698481	1727.289475	17.460263
38.049302	1743.018794	17.465280
37.981441	1757.882102	17.470298
38.193856	1761.782372	17.475315
38.124802	1758.867581	17.480333
38.055595	1767.201499	17.485351
38.455657	1760.957306	17.490368
38.348224	1762.338268	17.495386
38.247008	1767.764054	17.500403
38.468409	1754.378520	17.505421
38.428522	1767.245930	17.510439
38.401217	1758.601824	17.515456
38.309317	1764.600276	17.520474
38.259955	1760.000783	17.525491
38.723251	1769.328870	17.530509
39.033063	1773.761021	17.535527
39.130627	1764.412731	17.540544
39.236753	1761.676067	17.545562
38.833633	1760.645553	17.550579
39.141115	1757.592059	17.555597
38.891715	1750.087640	17.560615
38.804209	1745.755356	17.565632
39.046285	1758.571498	17.570650
39.146901	1748.271054	17.575667
39.042047	1746.968029	17.580685
38.577783	1760.247607	17.585703
39.260236	1744.738903	17.590720
39.050789	1741.569654	17.595738
39.005039	1759.649411	17.600755
39.389706	1747.357836	17.605773
39.231251	1747.710313	17.610791
39.186401	1741.170572	17.615808
39.325871	1754.006220	17.620826
39.193350	1749.336623	17.625843
39.565404	1750.037072	17.630861
39.053899	1752.885612	17.635879
39.438711	1762.407109	17.640896
39.662501	1761.317510	17.645914
39.579070	1753.258085	17.650931
39.555712	1741.080353	17.655949
39.424544	1758.840251	17.660967
39.792460	1756.019365	17.665984
39.570538	1763.183713	17.671002
39.830996	1771.405282	17.676019
40.178876	1768.345343	17.681037
39.652085	1761.303582	17.686055
39.961876	1743.738598	17.691072
39.272792	1748.817687	17.696090
39.336486	1751.620108	17.701107
39.621299	1774.347352	17.706125
39.774437	1779.940217	17.711143
39.802262	1769.770915	17.716160
40.035590	1788.501476	17.721178
39.732534	1770.493078	17.726195
40.248657	1773.226494	17.731213
39.942539	1775.768576	17.736231
40.172959	1773.202423	17.741248
40.268867	1773.707815	17.746266
40.135311	1770.605108	17.751283
40.381490	1775.983358	17.756301
40.810505	1769.945329	17.761319
40.398231	1776.657124	17.766336
40.447813	1764.124821	17.771354
40.569763	1768.012778	17.776371
40.561608	1763.400420	17.781389
40.559191	1766.005749	17.786407
40.711893	1772.260923	17.791424
40.912673	1757.077562	17.796442
40.428713	1759.797441	17.801459
40.543270	1774.888077	17.806477
40.284075	1760.188631	17.811495
40.628597	1762.217958	17.816512
40.507348	1771.066692	17.821530
40.142036	1776.393028	17.826547
40.880675	1783.476551	17.831565
40.978669	1794.286501	17.836583
40.749494	1787.955460	17.841600
40.912357	1788.607478	17.846618
40.983195	1798.946709	17.851635
40.811868	1790.648024	17.856653
40.808548	1799.517292	17.861671
41.154823	1784.205307	17.866688
40.912458	1785.620375	17.871706
40.641255	1798.905377	17.876723
41.063846	1803.824493	17.881741
41.400899	1814.726895	17.886759
41.631287	1819.555546	17.891776
41.214104	1806.775177	17.896794
41.329097	1826.100387	17.901811
41.518488	1818.382806	17.906829
41.716016	1827.712418	17.911847
41.876546	1804.972302	17.916864
41.291266	1788.619672	17.921882
41.283380	1801.960210	17.926899
41.671979	1794.737835	17.931917
41.559091	1816.620937	17.936935
41.628904	1811.377928	17.941952
41.511863	1827.314091	17.946970
41.956193	1816.436535	17.951987
42.028597	1809.716040	17.957005
41.764254	1816.276845	17.962023
42.116449	1810.358017	17.967040
41.927123	1817.087756	17.972058
41.700870	1814.894876	17.977075
42.180610	1809.119303	17.982093
42.033406	1816.899399	17.987111
42.042368	1818.175286	17.992128
41.903043	1816.465619	17.997146
41.990694	1825.812754	18.002163
42.217449	1816.564950	18.007181
42.262344	1824.597559	18.012199
42.206278	1815.465647	18.017216
42.227865	1813.525824	18.022234
42.365658	1817.892615	18.027251
42.542209	1819.838627	18.032269
42.324499	1823.061896	18.037287
42.222826	1825.502167	18.042304
41.801433	1822.769397	18.047322
41.885654	1821.400032	18.052339
42.084214	1835.288123	18.057357
42.089188	1840.159024	18.062375
42.551010	1851.741554	18.067392
42.630182	1848.232094	18.072410
42.530657	1851.090453	18.077427
42.525555	1850.419600	18.082445
42.736234	1843.497711	18.087463
42.657346	1850.584234	18.092480
43.101556	1853.359024	18.097498
43.166239	1864.459058	18.102515
42.895948	1853.099266	18.107533
42.450746	1863.179495	18.112551
42.891091	1865.689060	18.117568
43.417762	1878.164190	18.122586
43.204550	1880.689899	18.127603
43.449571	1864.577573	18.132621
43.341100	1877.317592	18.137639
43.451396	1870.715296	18.142656
43.453982	1876.756928	18.147674
43.561674	1865.531900	18.152691
43.466315	1841.268942	18.157709
43.543639	1839.335956	18.162727
43.638760	1836.143282	18.167744
43.599426	1827.362626	18.172762
42.914840	1839.060338	18.177779
43.582611	1842.158122	18.182797
43.720435	1856.272998	18.187815
43.561905	1856.730882	18.192832
43.736290	1839.929849	18.197850
43.887996	1863.611269	18.202867
43.656015	1850.507167	18.207885
43.688526	1862.617499	18.212903
43.755188	1871.942842	18.217920
43.655305	1866.774068	18.222938
43.437588	1872.452855	18.227955
43.939679	1865.869874	18.232973
44.229457	1870.074015	18.237991
43.953816	1872.936871	18.243008
43.889065	1867.171033	18.248026
43.944568	1872.597032	18.253043
44.246405	1869.545989	18.258061
44.207563	1872.260967	18.263079
44.239800	1859.080112	18.268096
44.559387	1869.530734	18.273114
44.061725	1875.853494	18.278131
43.959508	1871.773632	18.283149
44.164973	1871.531667	18.288167
44.320500	1884.528467	18.293184
44.718056	1895.573865	18.298202
44.612152	1895.855042	18.303219
44.274242	1898.814351	18.308237
44.213679	1896.494359	18.313255
44.460748	1889.521027	18.318272
44.816163	1894.647518	18.323290
44.625260	1890.295501	18.328307
44.764303	1890.325254	18.333325
44.964060	1886.492958	18.338343
44.709204	1895.805098	18.343360
45.137866	1881.755605	18.348378
44.934730	1894.713658	18.353395
45.206507	1883.355482	18.358413
45.246842	1878.714904	18.363431
45.185584	1897.031687	18.368448
44.998544	1879.481281	18.373466
44.670092	1891.366057	18.378483
44.970835	1893.647779	18.383501
45.121115	1896.235071	18.388519
45.127969	1900.706141	18.393536
45.486796	1919.026743	18.398554
45.329191	1930.319583	18.403571
45.392841	1909.938585	18.408589
45.689521	1915.930183	18.413607
45.630833	1914.440454	18.418624
46.009973	1910.554375	18.423642
45.593212	1914.248287	18.428659
45.914130	1914.118472	18.433677
46.008391	1901.213980	18.438695
45.814951	1893.359212	18.443712
45.666530	1877.271865	18.448730
45.425860	1885.897467	18.453747
45.668928	1897.230201	18.458765
45.475375	1905.461333	18.463783
45.499241	1915.981173	18.468800
45.637148	1907.939845	18.473818
45.558558	1919.468615	18.478835
45.826773	1914.733481	18.483853
45.875625	1904.532417	18.488871
45.955150	1922.523184	18.493888
46.582790	1920.351411	18.498906
46.345225	1930.390706	18.503923
46.606465	1919.089239	18.508941
46.337868	1912.495440	18.513959
46.393614	1902.865864	18.518976
46.517152	1911.700812	18.523994
46.136336	1893.979943	18.529011
46.229971	1908.952931	18.534029
46.507989	1926.087774	18.539047
46.361918	1939.488229	18.544064
46.532626	1928.262541	18.549082
46.140524	1950.898243	18.554099
46.537132	1932.787497	18.559117
46.638984	1943.880091	18.564135
46.753605	1936.849208	18.569152
46.439571	1935.448964	18.574170
46.442819	1951.504506	18.579187
46.737638	1951.751665	18.584205
46.985019	1970.017745	18.589223
46.979275	1960.528500	18.594240
47.125397	1963.298940	18.599258
47.028659	1975.393799	18.604275
47.280239	1966.491158	18.609293
47.870570	1970.670992	18.614311
47.425719	1967.954519	18.619328
47.422662	1959.289122	18.624346
47.482661	1957.904731	18.629363
47.393107	1951.770003	18.634381
47.299829	1935.365481	18.639399
47.553111	1952.037107	18.644416
47.494355	1953.097288	18.649434
47.378453	1967.299928	18.654451
47.555427	1960.048302	18.659469
47.841906	1966.815487	18.664487
47.917439	1965.151761	18.669504
47.893580	1954.955966	18.674522
47.824510	1949.609214	18.679539
47.933100	1963.958522	18.684557
48.086615	1951.857799	18.689575
47.967240	1951.736854	18.694592
48.140592	1936.508917	18.699610
47.702502	1929.666859	18.704627
47.936586	1953.395064	18.709645
47.985855	1951.131480	18.714663
47.842318	1970.482383	18.719680
48.161528	1954.587790	18.724698
48.032504	1966.637453	18.729715
48.125969	1961.061853	18.734733
48.343115	1963.940518	18.739751
48.216915	1953.350480	18.744768
48.273862	1961.486637	18.749786
47.880426	1959.205564	18.754803
48.014460	1955.813173	18.759821
48.132495	1968.092427	18.764839
48.228823	1975.316237	18.769856
48.320254	1980.165531	18.774874
48.436872	1984.800022	18.779891
48.392674	1977.267477	18.784909
48.318276	1975.097545	18.789927
48.572318	1984.500044	18.794944
48.783332	1988.101721	18.799962
49.138006	1999.265724	18.804979
48.956093	1992.299409	18.809997
49.090422	1979.893406	18.815015
48.705898	1992.259120	18.820032
49.234142	1993.818728	18.825050
49.385979	1992.831825	18.830067
49.470410	1996.049418	18.835085
49.665864	1976.713832	18.840103
49.255197	1977.276426	18.845120
49.149939	1961.885253	18.850138
49.288359	1965.312882	18.855155
49.230582	1956.319582	18.860173
49.508906	1974.225225	18.865191
49.189088	1990.146714	18.870208
49.475530	1996.976841	18.875226
49.638177	2002.867155	18.880243
49.559376	1997.575420	18.885261
49.885016	2000.098585	18.890279
49.497113	2005.338942	18.895296
49.837162	1999.494336	18.900314
49.764276	1992.584566	18.905331
49.511706	2005.764537	18.910349
50.110417	1992.367375	18.915367
49.739959	2003.002076	18.920384
49.869085	2005.824000	18.925402
49.860953	1992.606989	18.930419
49.253625	2001.036300	18.935437
49.840689	2021.197279	18.940455
49.852465	2028.003584	18.945472
50.195626	2024.790187	18.950490
50.182858	2025.942141	18.955507
50.081058	2034.687258	18.960525
50.521071	2029.169623	18.965543
50.191338	2030.733929	18.970560
50.229784	2026.508892	18.975578
50.411533	2025.492048	18.980595
50.245490	2045.889573	18.985613
50.517319	2044.262174	18.990631
50.722525	2054.219930	18.995648
51.148724	2059.844862	19.000666
51.038024	2056.367206	19.005683
50.752579	2058.149399	19.010701
51.171419	2044.321544	19.015719
50.949963	2034.836765	19.020736
50.718657	2024.364113	19.025754
50.897272	2028.096811	19.030771
51.134771	2039.315713	19.035789
51.352340	2046.457301	19.040807
51.098370	2054.408709	19.045824
51.295325	2053.612812	19.050842
51.331099	2041.195732	19.055859
51.033230	2055.680740	19.060877
51.488707	2046.323954	19.065895
51.376332	2047.833148	19.070912
51.464498	2051.514208	19.075930
51.517208	2046.487778	19.080947
51.732983	2050.227140	19.085965
51.778498	2046.309288	19.090983
51.430979	2051.558951	19.096000
51.473815	2044.355417	19.101018
51.633228	2047.806459	19.106035
51.216042	2043.547113	19.111053
51.593980	2037.834878	19.116071
51.330319	2049.453043	19.121088
51.488416	2035.311269	19.126106
51.760468	2055.382533	19.131123
51.668632	2063.718657	19.136141
51.951837	2070.563493	19.141159
51.986945	2072.621761	19.146176
52.110200	2074.549566	19.151194
51.891156	2077.321635	19.156211
51.975649	2079.222588	19.161229
52.352573	2068.929762	19.166247
52.096564	2071.399406	19.171264
52.047901	2073.076197	19.176282
52.247468	2080.566746	19.181299
52.505267	2101.426875	19.186317
52.882868	2093.781382	19.191335
52.525189	2107.075736	19.196352
52.837748	2102.498641	19.201370
52.993916	2098.627623	19.206387
52.726258	2101.608802	19.211405
52.895909	2094.446368	19.216423
52.990618	2104.127618	19.221440
52.695412	2097.435729	19.226458
53.123396	2094.244970	19.231475
53.157876	2100.926562	19.236493
53.233925	2097.261809	19.241511
53.078519	2101.537016	19.246528
53.616784	2092.838694	19.251546
53.425773	2080.061337	19.256563
53.066302	2075.259511	19.261581
53.301550	2077.652384	19.266599
53.221856	2088.399655	19.271616
53.182560	2091.797453	19.276634
53.262789	2092.816602	19.281651
53.037486	2095.275061	19.286669
53.371327	2089.058595	19.291687
53.312036	2095.821208	19.296704
53.231375	2087.223168	19.301722
53.451448	2084.455688	19.306739
53.694426	2102.068245	19.311757
53.555347	2107.311428	19.316775
53.916903	2112.965567	19.321792
53.772564	2121.281782	19.326810
54.487774	2107.672450	19.331827
54.074090	2120.127868	19.336845
54.354275	2110.748659	19.341863
54.214590	2099.770546	19.346880
53.880882	2096.325299	19.351898
54.465879	2092.720956	19.356915
54.364316	2101.101125	19.361933
54.451144	2099.467044	19.366951
54.046776	2092.912118	19.371968
53.961012	2115.302587	19.376986
54.269577	2094.750134	19.382003
54.416265	2118.709631	19.387021
54.474482	2115.134235	19.392039
54.392628	2108.342246	19.397056
54.423263	2106.161836	19.402074
54.580375	2100.862329	19.407091
54.526800	2117.326674	19.412109
54.571279	2114.978883	19.417127
54.522416	2134.096249	19.422144
54.761874	2138.684457	19.427162
55.036872	2139.614345	19.432179
54.723979	2142.576004	19.437197
55.142601	2142.562744	19.442215
55.020644	2143.894146	19.447232
54.612637	2146.521754	19.452250
54.848958	2139.949576	19.457267
55.023151	2154.063662	19.462285
54.917589	2172.175493	19.467303
55.105492	2163.070524	19.472320
55.244010	2165.135910	19.477338
55.659912	2161.901445	19.482355
55.492133	2164.108489	19.487373
55.600561	2160.352037	19.492391
55.592013	2167.350416	19.497408
55.504006	2172.329068	19.502426
55.733776	2160.996252	19.507443
55.795356	2162.117483	19.512461
55.771613	2161.536107	19.517479
55.877491	2170.212004	19.522496
55.942819	2182.794009	19.527514
56.221125	2190.956342	19.532531
55.933933	2195.369001	19.537549
56.046788	2187.353537	19.542567
56.081321	2186.611851	19.547584
56.514422	2186.701679	19.552602
56.857048	2189.222169	19.557619
56.452846	2182.402900	19.562637
56.236042	2165.855791	19.567655
56.419157	2168.903524	19.572672
56.417158	2172.098759	19.577690
56.583176	2187.585896	19.582707
56.606574	2192.699376	19.587725
56.834574	2182.826634	19.592743
56.808582	2186.875155	19.597760
56.688864	2193.381602	19.602778
56.964146	2184.094366	19.607795
56.994264	2193.715188	19.612813
56.661133	2184.487226	19.617831
56.706113	2185.055814	19.622848
57.079215	2180.572862	19.627866
57.194321	2193.631443	19.632883
56.763762	2183.901479	19.637901
57.096006	2177.669500	19.642919
57.275419	2170.414235	19.647936
56.929262	2185.819451	19.652954
57.198539	2181.958689	19.657971
57.243239	2184.174323	19.662989
57.255521	2177.974494	19.668007
57.481995	2188.776834	19.673024
57.529253	2195.687674	19.678042
57.612686	2202.872754	19.683059
57.346615	2208.331287	19.688077
57.503491	2202.171311	19.693095
57.816347	2205.731631	19.698112
57.673388	2219.295447	19.703130
57.726798	2204.643225	19.708147
57.466101	2208.079505	19.713165
57.543744	2216.692291	19.718183
58.013180	2230.289805	19.723200
58.241302	2233.700833	19.728218
58.234418	2236.954279	19.733235
58.117890	2241.074671	19.738253
58.548726	2232.364298	19.743271
58.520178	2224.372151	19.748288
58.482560	2232.570733	19.753306
58.621105	2230.928390	19.758323
58.405723	2231.806710	19.763341
58.572876	2227.216585	19.768359
58.668885	2230.038329	19.773376
58.446297	2236.937951	19.778394
58.675192	2228.163042	19.783411
58.443122	2240.859380	19.788429
58.398380	2232.920936	19.793447
58.553782	2217.978721	19.798464
58.831420	2239.402978	19.803482
59.249842	2248.283131	19.808499
59.169404	2247.910573	19.813517
59.196222	2258.858854	19.818535
59.556465	2251.836627	19.823552
59.434084	2237.891189	19.828570
59.396810	2224.756482	19.833587
59.167610	2224.534281	19.838605
59.008774	2230.323369	19.843623
59.246123	2235.670952	19.848640
59.211617	2242.827669	19.853658
59.339747	2241.052488	19.858675
59.191760	2247.541444	19.863693
59.277260	2254.045865	19.868711
59.722972	2246.061446	19.873728
59.474408	2240.901305	19.878746
59.784899	2251.725688	19.883763
59.578064	2265.358723	19.888781
59.753340	2277.843049	19.893799
60.048008	2274.692391	19.898816
59.981566	2286.165243	19.903834
60.475347	2273.907739	19.908851
60.359105	2282.487774	19.913869
60.505089	2273.250203	19.918887
60.391818	2274.879117	19.923904
60.108778	2279.107088	19.928922
60.204330	2271.607161	19.933939
60.123121	2277.297369	19.938957
60.381315	2282.894912	19.943975
60.339565	2278.990127	19.948992
60.083975	2277.127480	19.954010
60.429945	2283.165644	19.959027
60.463256	2308.760661	19.964045
60.767334	2301.149596	19.969063
60.940451	2297.320656	19.974080
60.818503	2296.181548	19.979098
61.234790	2294.840983	19.984115
61.040377	2299.441803	19.989133
61.210132	2294.586178	19.994151
61.485201	2301.549617	19.999168
61.123459	2302.601511	20.004186
61.193834	2296.522933	20.009203
61.115210	2297.072696	20.014221
61.239609	2304.625687	20.019239
61.346526	2295.821424	20.024256
61.256337	2304.099218	20.029274
61.698688	2313.460891	20.034291
62.040096	2330.089010	20.039309
61.616378	2311.192297	20.044327
61.802143	2305.339927	20.049344
61.969151	2323.010488	20.054362
61.918779	2315.029637	20.059379
62.033750	2320.954427	20.064397
62.135255	2320.351497	20.069415
62.152135	2325.547077	20.074432
61.803379	2315.490147	20.079450
62.106795	2317.456110	20.084467
62.384562	2317.885329	20.089485
61.754148	2325.703428	20.094503
62.012330	2316.632775	20.099520
62.068602	2312.336382	20.104538
62.168198	2309.728077	20.109555
62.233930	2324.150646	20.114573
62.231929	2327.350635	20.119591
62.516262	2330.075510	20.124608
62.043103	2342.015977	20.129626
62.755964	2340.604515	20.134643
62.512496	2333.835835	20.139661
62.424843	2335.821693	20.144679
62.827959	2339.753059	20.149696
62.659674	2343.938365	20.154714
63.004317	2354.445122	20.159731
63.265476	2351.884980	20.164749
63.186100	2367.037835	20.169767
63.335828	2364.374333	20.174784
63.115305	2357.115112	20.179802
63.653133	2351.589625	20.184819
63.636474	2354.961851	20.189837
63.314479	2358.216811	20.194855
63.328910	2359.778962	20.199872
63.431472	2356.350598	20.204890
63.429423	2359.622963	20.209907
63.664501	2357.406766	20.214925
63.689436	2357.744167	20.219943
63.931248	2350.222448	20.224960
63.572295	2351.935383	20.229978
63.747133	2346.728132	20.234995
64.005595	2342.135208	20.240013
63.894985	2362.989971	20.245031
64.222355	2367.842669	20.250048
64.379291	2373.847308	20.255066
64.315242	2382.914602	20.260083
64.528507	2386.818054	20.265101
64.441641	2369.247932	20.270119
64.496874	2370.198725	20.275136
64.354314	2383.147551	20.280154
64.582814	2370.089097	20.285171
64.895769	2366.180420	20.290189
64.713072	2379.956010	20.295207
65.058238	2378.661388	20.300224
64.738974	2372.875373	20.305242
64.645443	2365.402406	20.310259
64.574946	2367.100803	20.315277
64.794757	2363.535757	20.320295
64.911938	2363.666530	20.325312
64.771631	2378.097628	20.330330
64.524266	2376.003199	20.335347
65.000931	2398.273735	20.340365
65.119403	2405.019941	20.345383
65.120326	2406.236599	20.350400
65.168009	2410.058706	20.355418
64.997327	2404.405506	20.360435
65.032427	2406.480341	20.365453
65.304122	2428.362809	20.370471
65.430796	2420.233324	20.375488
65.586226	2430.969307	20.380506
65.811796	2437.043255	20.385523
66.021960	2430.958845	20.390541
65.500383	2431.769597	20.395559
65.634203	2427.503277	20.400576
65.618651	2446.338090	20.405594
65.868802	2449.446769	20.410611
66.150992	2448.085102	20.415629
65.987798	2464.137079	20.420647
66.252270	2463.913227	20.425664
66.369650	2466.193610	20.430682
66.540415	2458.594285	20.435699
66.792390	2454.045621	20.440717
66.638653	2471.682567	20.445735
66.944036	2452.320955	20.450752
66.770278	2459.893259	20.455770
66.774288	2453.985655	20.460787
67.185593	2449.202361	20.465805
66.752056	2450.053346	20.470823
67.070970	2449.367761	20.475840
67.035792	2459.986291	20.480858
67.150571	2453.966636	20.485875
67.665564	2440.216675	20.490893
67.106839	2452.006487	20.495911
67.246620	2453.401574	20.500928
67.380563	2445.279568	20.505946
67.011716	2448.501905	20.510963
67.348529	2443.957019	20.515981
67.080833	2455.518730	20.520999
67.112550	2444.358072	20.526016
67.234987	2453.669389	20.531034
67.462382	2471.674223	20.536051
67.866518	2474.084278	20.541069
67.706556	2475.443007	20.546087
68.042000	2481.544285	20.551104
67.918337	2473.201424	20.556122
67.833087	2476.437531	20.561139
68.005333	2473.941886	20.566157
67.997102	2473.114980	20.571175
68.203485	2473.988190	20.576192
68.060236	2495.319490	20.581210
68.289687	2501.642183	20.586227
68.135821	2503.556034	20.591245
68.095656	2510.713785	20.596263
68.234546	2512.236441	20.601280
68.691857	2498.968341	20.606298
68.577451	2507.203706	20.611315
68.571121	2502.270696	20.616333
68.233527	2515.674693	20.621351
68.719747	2533.284380	20.626368
68.995164	2528.727235	20.631386
68.966203	2534.822937	20.636403
69.566521	2521.576058	20.641421
69.195421	2528.201397	20.646439
69.399333	2531.598267	20.651456
69.428698	2531.345838	20.656474
69.318144	2530.072752	20.661491
69.647074	2530.135152	20.666509
69.401876	2525.967001	20.671527
69.660026	2521.864880	20.676544
69.425084	2535.211624	20.681562
69.370042	2523.282907	20.686579
69.730396	2523.481088	20.691597
69.609075	2521.380694	20.696615
69.489585	2522.626788	20.701632
69.979439	2518.822003	20.706650
70.050730	2512.586665	20.711667
70.092638	2517.816863	20.716685
70.112071	2521.595525	20.721703
70.167746	2518.208422	20.726720
70.048545	2525.137312	20.731738
70.073834	2540.855705	20.736755
70.542503	2542.218803	20.741773
70.522118	2551.236765	20.746791
70.109910	2558.930521	20.751808
70.285116	2556.851264	20.756826
70.433175	2546.934394	20.761843
70.607364	2551.294031	20.766861
70.584246	2549.760809	20.771879
70.795571	2563.965333	20.776896
70.969445	2565.130039	20.781914
70.648086	2585.757592	20.786931
71.138677	2575.945749	20.791949
71.066266	2576.866572	20.796967
71.036823	2573.898106	20.801984
71.085450	2572.620868	20.807002
71.243539	2571.993174	20.812019
71.447902	2567.364760	20.817037
71.321418	2573.084327	20.822055
71.599172	2583.358872	20.827072
71.848194	2585.748062	20.832090
71.715925	2599.008488	20.837107
72.246323	2588.878025	20.842125
71.983634	2581.821267	20.847143
71.595821	2564.788925	20.852160
72.156510	2560.183132	20.857178
72.008797	2593.168883	20.862195
72.122464	2587.617352	20.867213
72.257067	2596.867042	20.872231
72.387316	2593.124304	20.877248
72.624372	2579.366623	20.882266
72.409151	2599.554103	20.887283
72.711430	2591.037849	20.892301
72.498464	2595.565425	20.897319
72.620430	2582.336570	20.902336
72.391076	2593.330675	20.907354
72.276504	2594.467446	20.912371
72.515129	2580.779517	20.917389
72.578807	2599.548408	20.922407
72.648567	2591.962762	20.927424
72.975451	2600.034993	20.932442
72.863080	2619.874172	20.937459
72.973857	2613.804750	20.942477
73.211696	2613.552896	20.947495
73.092958	2619.775428	20.952512
73.217392	2610.154095	20.957530
73.201993	2620.186750	20.962547
73.060563	2615.492335	20.967565
73.184240	2616.812137	20.972583
73.464835	2636.256745	20.977600
73.859339	2642.270018	20.982618
73.800969	2641.503010	20.987635
74.064797	2639.829632	20.992653
74.237298	2639.408861	20.997671
74.428840	2638.298388	21.002688
74.298432	2637.715912	21.007706
74.250049	2625.489516	21.012723
73.967915	2624.626837	21.017741
74.227349	2619.816583	21.022759
74.171670	2633.336188	21.027776
74.565879	2626.334324	21.032794
74.624607	2629.343000	21.037811
74.844868	2627.569599	21.042829
74.971172	2624.912145	21.047847
74.998943	2630.750289	21.052864
75.069911	2623.783455	21.057882
74.566742	2627.256138	21.062899
75.231719	2626.267594	21.067917
75.007463	2634.426948	21.072935
74.520662	2629.015205	21.077952
74.978773	2623.137368	21.082970
74.661270	2634.235229	21.087987
75.082709	2621.481642	21.093005
74.953986	2644.055965	21.098023
74.913345	2649.482643	21.103040
74.949796	2659.309629	21.108058
75.189248	2672.536013	21.113075
75.437077	2648.584301	21.118093
75.721118	2667.710631	21.123111
75.446540	2698.246266	21.128128
75.599258	2686.174951	21.133146
75.624506	2692.163754	21.138163
76.084561	2689.468797	21.143181
76.535358	2678.764192	21.148199
76.157450	2685.882288	21.153216
76.368903	2685.215403	21.158234
75.954241	2686.804329	21.163251
76.252092	2686.232999	21.168269
76.329508	2685.415232	21.173287
76.369403	2697.370917	21.178304
76.970855	2697.147598	21.183322
77.109563	2702.634577	21.188339
77.040542	2683.721713	21.193357
77.143442	2681.022361	21.198375
76.936152	2676.938575	21.203392
77.495287	2667.376879	21.208410
76.951688	2667.201659	21.213427
77.044279	2667.879085	21.218445
77.154216	2661.862476	21.223463
76.874936	2682.375696	21.228480
77.255381	2670.530004	21.233498
77.148285	2698.286756	21.238515
77.009213	2699.808925	21.243533
77.380833	2705.006276	21.248551
77.551287	2697.900052	21.253568
77.495157	2702.305902	21.258586
77.167964	2697.468041	21.263603
77.266867	2700.824278	21.268621
77.422184	2726.446194	21.273639
77.518527	2736.130753	21.278656
77.841306	2714.936471	21.283674
77.957874	2731.931265	21.288691
77.979641	2724.829862	21.293709
78.858711	2731.282671	21.298727
78.865579	2727.165506	21.303744
79.112110	2706.415220	21.308762
78.735712	2712.456283	21.313779
78.827257	2703.701419	21.318797
78.866984	2697.547332	21.323815
78.672327	2704.928028	21.328832
78.787015	2696.612313	21.333850
78.967053	2695.800991	21.338867
78.935795	2699.252708	21.343885
79.262232	2699.457088	21.348903
78.977521	2708.603034	21.353920
79.106600	2691.951398	21.358938
78.829733	2707.579722	21.363955
79.369529	2710.189209	21.368973
79.372425	2725.559781	21.373991
79.583159	2730.887410	21.379008
79.704860	2721.742311	21.384026
79.466064	2728.658906	21.389043
79.555240	2727.165963	21.394061
79.843424	2732.684177	21.399079
79.611825	2717.676528	21.404096
79.747255	2734.254584	21.409114
79.792704	2758.611193	21.414131
79.994746	2757.520274	21.419149
80.435763	2766.552886	21.424167
80.175020	2773.663351	21.429184
80.449095	2750.361709	21.434202
80.336037	2763.886653	21.439219
80.221074	2758.259037	21.444237
80.491969	2756.917237	21.449255
80.367764	2770.189117	21.454272
80.914898	2759.242560	21.459290
80.901052	2764.473086	21.464307
81.077344	2777.911000	21.469325
81.093207	2778.532235	21.474343
80.822379	2785.003262	21.479360
80.798306	2782.464935	21.484378
80.788138	2790.692490	21.489395
80.933984	2786.594833	21.494413
81.115498	2786.000364	21.499431
81.228236	2786.764251	21.504448
81.386936	2781.556273	21.509466
81.331468	2810.670485	21.514483
81.400436	2811.637209	21.519501
81.508048	2815.271315	21.524519
81.311031	2821.323932	21.529536
81.825688	2810.615341	21.534554
82.024242	2814.813859	21.539571
81.863718	2816.997819	21.544589
82.003263	2812.652604	21.549607
81.780176	2836.165702	21.554624
82.177733	2830.247101	21.559642
82.031014	2836.001459	21.564659
82.085996	2834.896231	21.569677
82.662301	2826.288950	21.574695
82.358370	2842.506154	21.579712
82.719909	2836.065506	21.584730
82.737705	2847.225683	21.589747
82.954391	2857.012263	21.594765
83.044338	2859.252249	21.599783
82.932899	2867.871190	21.604800
83.816876	2864.492716	21.609818
83.429550	2865.031948	21.614835
83.522451	2861.572757	21.619853
83.415868	2840.794427	21.624871
83.426370	2850.763331	21.629888
83.462359	2860.070604	21.634906
83.575592	2853.966082	21.639923
83.610812	2855.867916	21.644941
83.959742	2846.497726	21.649959
83.808237	2849.703580	21.654976
83.891920	2855.315017	21.659994
83.949640	2865.979596	21.665011
83.832426	2862.532673	21.670029
84.120119	2846.771136	21.675047
84.208627	2852.417199	21.680064
83.880579	2852.520656	21.685082
84.285961	2854.345371	21.690099
84.199035	2868.677199	21.695117
84.729639	2870.555885	21.700135
84.553449	2868.309235	21.705152
84.774966	2867.107443	21.710170
84.888893	2872.197287	21.715187
84.510084	2883.091950	21.720205
85.021661	2869.722834	21.725223
84.902229	2874.533690	21.730240
84.822923	2876.094327	21.735258
85.222551	2890.314765	21.740275
85.175407	2892.121978	21.745293
85.417538	2900.094627	21.750311
85.005744	2904.639845	21.755328
85.482872	2898.166579	21.760346
85.491220	2886.910986	21.765363
85.499481	2892.927752	21.770381
85.784513	2892.221596	21.775399
85.726616	2889.506159	21.780416
85.745372	2894.313863	21.785434
85.788355	2900.371502	21.790451
85.598449	2914.007948	21.795469
86.083275	2914.238989	21.800487
85.802778	2935.345048	21.805504
86.143008	2917.125663	21.810522
86.141398	2928.303943	21.815539
86.151128	2951.686498	21.820557
86.316716	2944.622619	21.825575
86.541734	2944.242234	21.830592
86.584818	2950.148069	21.835610
86.493300	2954.292990	21.840627
87.018174	2947.726352	21.845645
87.226082	2947.559497	21.850663
86.850118	2959.031109	21.855680
87.342166	2961.796922	21.860698
87.416434	2975.553333	21.865715
87.196379	2985.888671	21.870733
87.428073	2970.497756	21.875751
87.667905	2972.164041	21.880768
87.871980	2971.684740	21.885786
87.887011	2967.445072	21.890803
87.993081	2969.750150	21.895821
87.979990	2956.693515	21.900839
87.824514	2972.031394	21.905856
87.964143	2965.121095	21.910874
88.109900	2964.843805	21.915891
87.958307	2963.279112	21.920909
87.833525	2954.151935	21.925927
88.219647	2975.382216	21.930944
88.444670	2973.774770	21.935962
88.463083	2997.470645	21.940979
88.723049	2993.123479	21.945997
88.859659	2980.993137	21.951015
88.746909	2990.367474	21.956032
88.786274	2977.419656	21.961050
89.068763	2970.783113	21.966067
88.995361	2979.311890	21.971085
89.037536	2984.147352	21.976103
89.043426	2993.757624	21.981120
89.162744	3005.377613	21.986138
89.202487	3020.020539	21.991155
88.989367	3016.168841	21.996173
89.207342	3005.652936	22.001191
89.606520	3004.658776	22.006208
89.731965	3030.261608	22.011226
89.954435	3027.629650	22.016243
89.707659	3039.262423	22.021261
90.435522	3030.045641	22.026279
90.171286	3036.295484	22.031296
90.182437	3035.485906	22.036314
90.468795	3024.215765	22.041331
90.582484	3028.449116	22.046349
90.745655	3025.055766	22.051367
90.443349	3028.988122	22.056384
90.718947	3024.226286	22.061402
90.717478	3026.620100	22.066419
90.804240	3027.571416	22.071437
90.785952	3012.591585	22.076455
91.034238	3032.070981	22.081472
90.601175	3028.408521	22.086490
90.991694	3027.072006	22.091507
90.924216	3029.072831	22.096525
91.243827	3037.217260	22.101543
91.234625	3052.551563	22.106560
90.992273	3055.027842	22.111578
91.350709	3033.733810	22.116595
91.552799	3047.290566	22.121613
91.361595	3048.185526	22.126631
91.524568	3061.012293	22.131648
91.512356	3078.459074	22.136666
91.478113	3071.734554	22.141683
91.546165	3081.445092	22.146701
92.021324	3093.909046	22.151719
91.913223	3096.235710	22.156736
92.016794	3104.781962	22.161754
92.349988	3108.266903	22.166771
92.227962	3109.651102	22.171789
92.645659	3117.347314	22.176807
92.739674	3131.801571	22.181824
92.765474	3127.163701	22.186842
93.323134	3128.511097	22.191859
93.056853	3129.278808	22.196877
93.416095	3119.015600	22.201895
93.191857	3124.652646	22.206912
93.098277	3115.997062	22.211930
93.446100	3120.587184	22.216947
93.263961	3122.437977	22.221965
93.458466	3124.227136	22.226983
93.355177	3124.157886	22.232000
93.290329	3135.641377	22.237018
93.688739	3152.973214	22.242035
93.602926	3149.691119	22.247053
93.935668	3148.971051	22.252071
93.675812	3144.899447	22.257088
93.594397	3153.320268	22.262106
94.277044	3156.320807	22.267123
94.268751	3181.297869	22.272141
94.713074	3175.600571	22.277159
94.818985	3168.360466	22.282176
94.608943	3168.402630	22.287194
94.816322	3171.505703	22.292211
94.764396	3168.307084	22.297229
95.064403	3164.535558	22.302247
95.062287	3171.582949	22.307264
94.878688	3160.947693	22.312282
95.495762	3156.778724	22.317299
95.377922	3162.836161	22.322317
95.368659	3164.793111	22.327335
95.349951	3177.387805	22.332352
95.366041	3192.361110	22.337370
95.556393	3190.651407	22.342387
95.446922	3207.294227	22.347405
95.741127	3191.499031	22.352423
95.877289	3194.751905	22.357440
95.834262	3191.539276	22.362458
95.869676	3194.377165	22.367475
96.026889	3201.244992	22.372493
95.870523	3221.593061	22.377511
96.198122	3217.651938	22.382528
96.376664	3222.817340	22.387546
96.340201	3226.803319	22.392563
96.383729	3232.041382	22.397581
96.086504	3236.825646	22.402599
96.709027	3256.246452	22.407616
96.396558	3257.188291	22.412634
96.993918	3243.714701	22.417651
97.104442	3245.406357	22.422669
97.163951	3253.371352	22.427687
97.622458	3271.505511	22.432704
97.142603	3282.377252	22.437722
97.467544	3272.673955	22.442739
97.675244	3278.970568	22.447757
97.838212	3273.448672	22.452775
97.803460	3260.146656	22.457792
97.832279	3279.099752	22.462810
98.106255	3270.696956	22.467827
98.461263	3269.320462	22.472845
98.295228	3277.373350	22.477863
98.226781	3277.162463	22.482880
98.080950	3274.196681	22.487898
98.481367	3281.164205	22.492915
98.510316	3309.717696	22.497933
98.399215	3289.640302	22.502951
98.997102	3299.873748	22.507968
98.924403	3297.534228	22.512986
98.889155	3298.452315	22.518003
99.050854	3297.304865	22.523021
99.263134	3288.094626	22.528039
99.127905	3297.227326	22.533056
98.999811	3293.101632	22.538074
99.486829	3302.334907	22.543091
99.439850	3327.149270	22.548109
99.661808	3322.869423	22.553127
99.921574	3326.206447	22.558144
99.825468	3329.940816	22.563162
99.976731	3322.565975	22.568179
100.048354	3324.423523	22.573197
99.857215	3320.303154	22.578215
100.027082	3314.128842	22.583232
100.012616	3330.091978	22.588250
100.483310	3331.001758	22.593267
100.419424	3354.493449	22.598285
100.523065	3347.024718	22.603303
100.707071	3342.696643	22.608320
100.543171	3346.285293	22.613338
100.724522	3343.530047	22.618355
100.783586	3349.722964	22.623373
100.613560	3338.102168	22.628391
101.367679	3362.671646	22.633408
101.050478	3362.193651	22.638426
101.509651	3360.972803	22.643443
101.076380	3378.388760	22.648461
101.130645	3360.014630	22.653479
101.718804	3365.412886	22.658496
101.099844	3376.402842	22.663514
101.334738	3386.815370	22.668531
101.819629	3388.264069	22.673549
101.958887	3396.632537	22.678567
102.286236	3397.993089	22.683584
101.992496	3399.926213	22.688602
102.095659	3402.980666	22.693619
102.020341	3422.973134	22.698637
102.316133	3435.410922	22.703655
102.737903	3418.616608	22.708672
102.800822	3422.644216	22.713690
103.157745	3422.057936	22.718707
103.190947	3417.230010	22.723725
103.272986	3411.880647	22.728743
103.359129	3403.985980	22.733760
103.348965	3415.880230	22.738778
103.521948	3407.440758	22.743795
103.618375	3408.457420	22.748813
103.545832	3402.202948	22.753831
103.815134	3419.268583	22.758848
103.700157	3430.772885	22.763866
103.631462	3435.832265	22.768883
104.068129	3440.559351	22.773901
103.967657	3434.985797	22.778919
104.021590	3436.708525	22.783936
103.701347	3438.380008	22.788954
104.141098	3442.108405	22.793971
104.304286	3452.185522	22.798989
104.075194	3467.597800	22.804007
104.238003	3457.430968	22.809024
104.486152	3473.485321	22.814042
104.560612	3480.845518	22.819059
104.692635	3487.934600	22.824077
104.645915	3487.862621	22.829095
105.209805	3485.972184	22.834112
104.976088	3499.817531	22.839130
105.340681	3510.887519	22.844147
105.537116	3514.679905	22.849165
105.347617	3533.779055	22.854183
105.929740	3509.164582	22.859200
105.659153	3526.214172	22.864218
105.494716	3517.137801	22.869235
105.865286	3519.153009	22.874253
106.117525	3527.790648	22.879271
106.513336	3533.203121	22.884288
106.235170	3544.589585	22.889306
106.540184	3535.721524	22.894323
106.449015	3544.214920	22.899341
106.396945	3541.226266	22.904359
106.941845	3532.606281	22.909376
107.018062	3536.081961	22.914394
106.802908	3530.369336	22.919411
107.172201	3531.875815	22.924429
107.183689	3534.232248	22.929447
107.363186	3520.828970	22.934464
106.943379	3526.388802	22.939482
106.964565	3532.420289	22.944499
107.481317	3548.081854	22.949517
107.707850	3551.586271	22.954535
107.969284	3553.644845	22.959552
107.831595	3555.469724	22.964570
108.179833	3555.818529	22.969587
108.319326	3549.146320	22.974605
108.331177	3557.075030	22.979623
108.805926	3542.090767	22.984640
108.392623	3556.158308	22.989658
108.628930	3544.855633	22.994675
108.700454	3551.768754	22.999693
108.442261	3553.705668	23.004711
108.665994	3565.127748	23.009728
108.718972	3570.749864	23.014746
109.031038	3570.800021	23.019763
109.135180	3576.052927	23.024781
109.174580	3578.979928	23.029799
109.171616	3576.291001	23.034816
108.985550	3581.609064	23.039834
109.311688	3597.076892	23.044851
109.393613	3601.703276	23.049869
109.305078	3606.203452	23.054887
109.814684	3609.439349	23.059904
109.986566	3628.398404	23.064922
110.208634	3631.326180	23.069939
110.083706	3633.408615	23.074957
110.379627	3635.880966	23.079975
110.370859	3626.065461	23.084992
110.535305	3628.126139	23.090010
110.447225	3633.158787	23.095027
110.733035	3644.830614	23.100045
110.463002	3640.206715	23.105063
110.776736	3656.105289	23.110080
110.811689	3659.648147	23.115098
111.079431	3669.303637	23.120115
111.074631	3674.294702	23.125133
111.086548	3676.000560	23.130151
111.257884	3687.217132	23.135168
111.540075	3700.700368	23.140186
111.393041	3699.534468	23.145203
112.011862	3691.612918	23.150221
111.970586	3694.312103	23.155239
112.178667	3685.371308	23.160256
112.052956	3682.512359	23.165274
111.938031	3701.277324	23.170291
112.003981	3697.044271	23.175309
112.086896	3714.868378	23.180327
112.402875	3717.575104	23.185344
112.606385	3721.684209	23.190362
112.350356	3722.779906	23.195379
112.631835	3720.199773	23.200397
112.996001	3736.849479	23.205415
113.405787	3744.388392	23.210432
113.449206	3737.554427	23.215450
113.718882	3729.591776	23.220467
113.723667	3731.081671	23.225485
113.594256	3742.399731	23.230503
113.908709	3729.053405	23.235520
113.871633	3747.432372	23.240538
113.705065	3734.219379	23.245555
114.364967	3719.181815	23.250573
114.183142	3731.533972	23.255591
114.080963	3727.309628	23.260608
114.447871	3723.889924	23.265626
114.436952	3718.556846	23.270643
114.684513	3737.982239	23.275661
114.529340	3751.591113	23.280679
114.730344	3731.335912	23.285696
114.990014	3759.357136	23.290714
114.912875	3750.259620	23.295731
115.052127	3740.288284	23.300749
114.756159	3759.025554	23.305767
115.181791	3773.180571	23.310784
115.113796	3773.497426	23.315802
115.326314	3768.864190	23.320819
115.641602	3776.302556	23.325837
115.781727	3790.730448	23.330855
115.990539	3785.590428	23.335872
115.839199	3811.760296	23.340890
115.836568	3812.239786	23.345907
116.340679	3805.469989	23.350925
116.458565	3818.076492	23.355943
116.697470	3812.657134	23.360960
116.635424	3808.858221	23.365978
116.733124	3803.061778	23.370995
117.021315	3797.673897	23.376013
116.683124	3811.794994	23.381031
116.821790	3822.310493	23.386048
117.111922	3826.229613	23.391066
117.005020	3819.360583	23.396083
117.484925	3818.655567	23.401101
117.484812	3811.645226	23.406119
117.326863	3823.332891	23.411136
117.367134	3835.965945	23.416154
117.786423	3848.724218	23.421171
118.041542	3837.112322	23.426189
118.031781	3847.170879	23.431207
118.203662	3835.531352	23.436224
118.365927	3831.113779	23.441242
118.334611	3841.988352	23.446259
118.321060	3843.091803	23.451277
118.390150	3863.499209	23.456295
118.754911	3864.576164	23.461312
118.591051	3874.193630	23.466330
118.714899	3867.972933	23.471347
119.058323	3857.290105	23.476365
119.048512	3875.996841	23.481383
119.416229	3886.068391	23.486400
119.720457	3896.808479	23.491418
119.548158	3898.391131	23.496435
119.715519	3891.154244	23.501453
119.638309	3894.405900	23.506471
119.906013	3894.349860	23.511488
119.897301	3893.021081	23.516506
119.747932	3894.152486	23.521523
120.031794	3890.436056	23.526541
119.997403	3910.867108	23.531559
120.206947	3905.853577	23.536576
120.382563	3920.403372	23.541594
120.309780	3924.295431	23.546611
120.649386	3932.875330	23.551629
120.302128	3947.246577	23.556647
120.649967	3951.925067	23.561664
121.010820	3967.505749	23.566682
120.897697	3965.157621	23.571699
121.324400	3964.250266	23.576717
121.283303	3983.820342	23.581735
121.812716	3993.859891	23.586752
122.164134	4001.696154	23.591770
122.236957	4000.528997	23.596787
122.841224	3997.592136	23.601805
122.883406	3995.085512	23.606823
122.564077	3987.952926	23.611840
122.531089	3970.739638	23.616858
122.658039	3995.342543	23.621875
122.891549	3990.767249	23.626893
122.862533	3999.379219	23.631911
122.894008	3998.398794	23.636928
123.112949	3988.952639	23.641946
122.745732	3991.913093	23.646963
123.502746	3980.453900	23.651981
123.166415	3994.179987	23.656999
122.968913	4006.995842	23.662016
123.488483	3998.892511	23.667034
123.242303	4007.077359	23.672051
123.819421	4017.111679	23.677069
123.567378	4026.830621	23.682087
124.043190	4033.589044	23.687104
124.325165	4030.295303	23.692122
124.295715	4049.364884	23.697139
124.345300	4038.091604	23.702157
124.538455	4038.323559	23.707175
124.511378	4046.448320	23.712192
124.811093	4041.997755	23.717210
124.934737	4037.320397	23.722227
125.477968	4057.066429	23.727245
124.986491	4076.820145	23.732263
125.404430	4069.614800	23.737280
125.440298	4064.428316	23.742298
125.167178	4066.884494	23.747315
125.701648	4066.837049	23.752333
125.775801	4061.208665	23.757351
125.828166	4062.871934	23.762368
126.045072	4083.462176	23.767386
126.129418	4091.785522	23.772403
126.268525	4085.726708	23.777421
125.983864	4095.867027	23.782439
125.772746	4104.811736	23.787456
126.454281	4104.856478	23.792474
126.593786	4115.343736	23.797491
126.567840	4119.303109	23.802509
126.605368	4122.625410	23.807527
127.254657	4137.240704	23.812544
127.877985	4140.978561	23.817562
127.323339	4143.744737	23.822579
127.617945	4137.248122	23.827597
127.705544	4140.644255	23.832615
127.569342	4142.634162	23.837632
128.054634	4137.501068	23.842650
127.640993	4136.067705	23.847667
127.916257	4139.279733	23.852685
128.157501	4165.867486	23.857703
128.554502	4165.906466	23.862720
128.628874	4166.072406	23.867738
128.128980	4170.390553	23.872755
128.819820	4158.805686	23.877773
128.739706	4178.697687	23.882791
128.915981	4198.390718	23.887808
128.882234	4189.674611	23.892826
129.137383	4201.321882	23.897843
129.306031	4186.028638	23.902861
129.656678	4201.187985	23.907879
129.566700	4212.751845	23.912896
129.679346	4216.170747	23.917914
129.560304	4231.353098	23.922931
129.729284	4214.332300	23.927949
129.717557	4233.492119	23.932967
129.922803	4242.363444	23.937984
130.618131	4255.839534	23.943002
130.029549	4248.765484	23.948019
130.499981	4260.037071	23.953037
130.782783	4267.760915	23.958055
130.846456	4269.442070	23.963072
130.954629	4285.764285	23.968090
130.914997	4281.063324	23.973107
131.441597	4264.805920	23.978125
131.203592	4260.581838	23.983143
131.297023	4284.541590	23.988160
131.519093	4289.971827	23.993178
131.402653	4307.333641	23.998195
131.447856	4306.379327	24.003213
131.856206	4312.509093	24.008231
132.002180	4319.327322	24.013248
132.215457	4322.159884	24.018266
132.259696	4331.239438	24.023283
132.725855	4329.400672	24.028301
132.881940	4319.676414	24.033319
132.691503	4320.541431	24.038336
132.908901	4336.730650	24.043354
133.069886	4345.303875	24.048371
133.074245	4349.890158	24.053389
132.976441	4354.936403	24.058407
133.335053	4355.593521	24.063424
133.656326	4358.932780	24.068442
133.746624	4372.944400	24.073459
133.848749	4372.711018	24.078477
133.834503	4367.515898	24.083495
133.623705	4375.957263	24.088512
134.251313	4387.955142	24.093530
134.492179	4397.987489	24.098547
134.574514	4399.567352	24.103565
134.611895	4392.092136	24.108583
134.819534	4393.674832	24.113600
135.008364	4401.707939	24.118618
135.026044	4417.958985	24.123635
135.084472	4411.666678	24.128653
135.444987	4420.474022	24.133671
135.440144	4427.979499	24.138688
135.629136	4413.720373	24.143706
135.662076	4423.999074	24.148723
136.094958	4433.402185	24.153741
135.950483	4455.262807	24.158759
136.115754	4443.874010	24.163776
136.287507	4452.063266	24.168794
136.149948	4454.870767	24.173811
136.217846	4447.704533	24.178829
136.605312	4454.877650	24.183847
136.507547	4469.659592	24.188864
137.100930	4468.615503	24.193882
136.856558	4469.122545	24.198899
137.500096	4475.382440	24.203917
137.295752	4482.609811	24.208935
137.477186	4496.956295	24.213952
137.620814	4492.639829	24.218970
137.799884	4504.442644	24.223987
137.822270	4500.091228	24.229005
138.596886	4495.167546	24.234023
138.211583	4499.740486	24.239040
138.218436	4501.775284	24.244058
138.392251	4498.268196	24.249075
138.296355	4505.317808	24.254093
138.629673	4522.273049	24.259111
138.369309	4528.631462	24.264128
138.780200	4519.922143	24.269146
139.052135	4529.439871	24.274163
138.995741	4526.858408	24.279181
139.152961	4561.971945	24.284199
139.004636	4555.364051	24.289216
139.614178	4561.701776	24.294234
139.547496	4548.985023	24.299251
139.935563	4576.086615	24.304269
139.812921	4577.111542	24.309287
140.017554	4577.136359	24.314304
140.057964	4584.672461	24.319322
140.123858	4592.795288	24.324339
140.333655	4613.171077	24.329357
140.638135	4617.482245	24.334375
140.643991	4611.225768	24.339392
141.037570	4610.382661	24.344410
140.900081	4614.301739	24.349427
141.033616	4617.933738	24.354445
141.323547	4625.917809	24.359463
141.481184	4639.579108	24.364480
141.525341	4626.740776	24.369498
141.296012	4643.641120	24.374515
141.265623	4645.754250	24.379533
141.778156	4644.749001	24.384551
141.996446	4673.083802	24.389568
142.440368	4663.342531	24.394586
142.557595	4680.662023	24.399603
142.531658	4674.803923	24.404621
142.962022	4685.608656	24.409639
142.697234	4701.107369	24.414656
143.235529	4699.050953	24.419674
143.389490	4702.362689	24.424691
143.225060	4699.323272	24.429709
143.845083	4704.512426	24.434727
144.218239	4696.653904	24.439744
144.089702	4705.378129	24.444762
143.747352	4707.319953	24.449779
144.002709	4713.798392	24.454797
144.098344	4717.286991	24.459815
144.262193	4728.891813	24.464832
144.672802	4730.438252	24.469850
144.845131	4719.395827	24.474867
144.705984	4733.170613	24.479885
145.195393	4751.297760	24.484903
145.230650	4749.494610	24.489920
145.341692	4761.490200	24.494938
145.237621	4762.542073	24.499955
145.359397	4765.622953	24.504973
145.606216	4745.842855	24.509991
145.415166	4774.558573	24.515008
145.892834	4787.203735	24.520026
145.943309	4791.743470	24.525043
145.952519	4798.781971	24.530061
146.305650	4784.523850	24.535079
146.385258	4803.721770	24.540096
146.691317	4811.786760	24.545114
146.990705	4825.061400	24.550131
146.811373	4827.443747	24.555149
147.158150	4813.017476	24.560167
146.752553	4825.025477	24.565184
147.177063	4817.770737	24.570202
147.460494	4829.498962	24.575219
147.396068	4852.556533	24.580237
147.614702	4846.086668	24.585255
147.566183	4849.942062	24.590272
147.899049	4860.270796	24.595290
148.027121	4870.966528	24.600307
148.119707	4874.177954	24.605325
148.372304	4867.701092	24.610343
148.249761	4884.487925	24.615360
148.525840	4877.958540	24.620378
148.936377	4894.334706	24.625395
148.939616	4894.493903	24.630413
149.186119	4902.153858	24.635431
149.444114	4916.902341	24.640448
149.531243	4912.458665	24.645466
149.765748	4917.472573	24.650483
149.738532	4922.125430	24.655501
150.380141	4913.031384	24.660519
149.961726	4924.846412	24.665536
150.304457	4942.287596	24.670554
150.625929	4938.039407	24.675571
150.466506	4946.999984	24.680589
150.923784	4946.466884	24.685607
150.586059	4945.048865	24.690624
150.671395	4976.398778	24.695642
151.136218	4974.236038	24.700659
151.365154	4980.342773	24.705677
151.464372	4983.310867	24.710695
151.360328	4981.865026	24.715712
151.693124	4999.664230	24.720730
151.882018	4985.588652	24.725747
152.046797	5011.726774	24.730765
152.166807	4991.767533	24.735783
152.135444	5008.828684	24.740800
152.237199	5028.779372	24.745818
152.425040	5032.225812	24.750835
152.375329	5035.435574	24.755853
153.048150	5040.322999	24.760871
152.947290	5041.401126	24.765888
152.971758	5049.822672	24.770906
153.533192	5053.199325	24.775923
153.615028	5080.055666	24.780941
153.936193	5076.285795	24.785959
153.780947	5077.687272	24.790976
154.366842	5073.408687	24.795994
154.419517	5075.844551	24.801011
154.479523	5068.399998	24.806029
154.343505	5074.967746	24.811047
154.070515	5075.908901	24.816064
154.725314	5092.190489	24.821082
154.892984	5091.901806	24.826099
154.994035	5115.373165	24.831117
155.097279	5114.695114	24.836135
155.449183	5108.458776	24.841152
155.360708	5106.695764	24.846170
155.436569	5118.105663	24.851187
155.376213	5146.017722	24.856205
155.901403	5141.845559	24.861223
155.635632	5135.519670	24.866240
155.882993	5156.599823	24.871258
156.471356	5165.746545	24.876275
156.604043	5168.239684	24.881293
156.678673	5152.113157	24.886311
156.767485	5168.404040	24.891328
156.882608	5188.932609	24.896346
157.143027	5192.682194	24.901363
157.252596	5189.772848	24.906381
157.584682	5191.520666	24.911399
157.310669	5214.827775	24.916416
157.827153	5215.283547	24.921434
158.149056	5222.661812	24.926451
157.755144	5231.615892	24.931469
157.999903	5234.593087	24.936487
158.128250	5247.337612	24.941504
158.446837	5247.491378	24.946522
158.735985	5260.396725	24.951539
158.763047	5271.015236	24.956557
158.864765	5278.779503	24.961575
159.047469	5281.448774	24.966592
158.877070	5281.297378	24.971610
159.851857	5296.710009	24.976627
159.627469	5301.175719	24.981645
159.869792	5287.022892	24.986663
159.884289	5297.077788	24.991680
159.962104	5322.683571	24.996698
160.483418	5328.087726	25.001715
160.284023	5328.987268	25.006733
160.578446	5319.205682	25.011751
160.812374	5331.251375	25.016768
160.818159	5347.156048	25.021786
161.423193	5347.006893	25.026803
161.369011	5349.633701	25.031821
161.581421	5348.953969	25.036839
161.728506	5345.566589	25.041856
161.864591	5355.168665	25.046874
162.499238	5353.038588	25.051891
162.315990	5369.898588	25.056909
162.623823	5360.632488	25.061927
162.592187	5374.429281	25.066944
162.399059	5370.728745	25.071962
162.648363	5374.185135	25.076979
162.869916	5365.781644	25.081997
163.111417	5372.484436	25.087015
162.963606	5372.405748	25.092032
163.190765	5382.462199	25.097050
163.474732	5400.784182	25.102067
163.340090	5405.253708	25.107085
163.609275	5399.415924	25.112103
163.810727	5406.769431	25.117120
163.967598	5417.962103	25.122138
164.476652	5418.688910	25.127155
164.537365	5418.753985	25.132173
164.347488	5413.800481	25.137191
164.668858	5435.486800	25.142208
164.361478	5444.394957	25.147226
165.133734	5442.064345	25.152243
165.069018	5443.497838	25.157261
165.122867	5463.764358	25.162279
165.413676	5469.276908	25.167296
165.286231	5475.090584	25.172314
165.901113	5477.204801	25.177331
165.764180	5487.591573	25.182349
166.231370	5495.401533	25.187367
166.397971	5496.757242	25.192384
166.633622	5516.009886	25.197402
166.703830	5521.294078	25.202419
166.577970	5532.055165	25.207437
166.802100	5524.658954	25.212455
167.239719	5549.098500	25.217472
167.028710	5555.328328	25.222490
167.645172	5558.736453	25.227507
167.797216	5560.096850	25.232525
167.812536	5572.581966	25.237543
168.515975	5578.985419	25.242560
168.418610	5584.551247	25.247578
168.580138	5578.895767	25.252595
168.504732	5575.694856	25.257613
168.404151	5580.007955	25.262631
168.522229	5597.302431	25.267648
168.603456	5607.945592	25.272666
168.850082	5615.476881	25.277683
169.321300	5618.426705	25.282701
169.428617	5629.972809	25.287719
169.551481	5624.089033	25.292736
169.897610	5638.915452	25.297754
170.239147	5657.024029	25.302771
170.115801	5666.421426	25.307789
170.158083	5676.038667	25.312807
170.538637	5666.887445	25.317824
170.826904	5686.072132	25.322842
170.802828	5689.636694	25.327859
171.286786	5696.573974	25.332877
170.944388	5692.352742	25.337895
171.211836	5692.847452	25.342912
171.471560	5708.720683	25.347930
171.788224	5714.288209	25.352947
171.985198	5719.869311	25.357965
171.884770	5708.018398	25.362983
172.188758	5709.513503	25.368000
172.040294	5738.587773	25.373018
172.136859	5734.572685	25.378035
172.596973	5735.985471	25.383053
172.461891	5748.460099	25.388071
172.972351	5753.234406	25.393088
172.831149	5772.529372	25.398106
173.392944	5764.464774	25.403123
173.301646	5791.464091	25.408141
173.766206	5795.950707	25.413159
173.891621	5794.783680	25.418176
174.109453	5799.398533	25.423194
174.163612	5811.852485	25.428211
174.435759	5829.743400	25.433229
174.637117	5821.335790	25.438247
174.688302	5823.593429	25.443264
174.819865	5833.943145	25.448282
175.498874	5836.985765	25.453299
175.256915	5854.555080	25.458317
175.479626	5851.780980	25.463335
175.782904	5849.463714	25.468352
175.721917	5858.716760	25.473370
176.085263	5876.889004	25.478387
176.233537	5888.877219	25.483405
176.095168	5884.270947	25.488423
176.342289	5884.948280	25.493440
176.163023	5906.774116	25.498458
176.248967	5913.955116	25.503475
176.180200	5920.293017	25.508493
176.028858	5936.567966	25.513511
176.976062	5957.212770	25.518528
177.108769	5969.508786	25.523546
177.490180	5984.821640	25.528563
177.827648	6004.227052	25.533581
178.218162	5999.622966	25.538599
178.520689	6007.029893	25.543616
178.196364	5999.901835	25.548634
178.762906	6010.412056	25.553651
178.864922	6023.876599	25.558669
179.259948	6034.497576	25.563687
179.433271	6023.243173	25.568704
179.437524	6035.345730	25.573722
179.605082	6048.755789	25.578739
179.888714	6050.487837	25.583757
179.775158	6056.066650	25.588775
179.967909	6049.685358	25.593792
179.999135	6069.934289	25.598810
180.557838	6075.177778	25.603827
180.762443	6081.471378	25.608845
180.633749	6090.381329	25.613863
180.901345	6069.851103	25.618880
181.135407	6080.526098	25.623898
181.496916	6094.153101	25.628915
181.332304	6104.794117	25.633933
181.566848	6112.289037	25.638951
182.011320	6108.045299	25.643968
181.540303	6114.858880	25.648986
182.076263	6125.163999	25.654003
182.179161	6134.845829	25.659021
182.127714	6143.118820	25.664039
182.672415	6140.184763	25.669056
182.542054	6152.843077	25.674074
182.936732	6157.881443	25.679092
182.950408	6167.961452	25.684109
182.754708	6169.335648	25.689127
183.184790	6189.352791	25.694144
183.324726	6200.510208	25.699162
183.872070	6219.309691	25.704180
183.999186	6211.906576	25.709197
183.961710	6230.870116	25.714215
184.766883	6229.083298	25.719232
184.699582	6242.995946	25.724250
184.898996	6240.009132	25.729268
184.888359	6252.617761	25.734285
185.301097	6252.360011	25.739303
185.776225	6266.633080	25.744320
185.494919	6278.846662	25.749338
185.715177	6274.914774	25.754356
186.023237	6270.289920	25.759373
186.035687	6301.833652	25.764391
186.261802	6293.930073	25.769408
186.498143	6291.364569	25.774426
186.636729	6308.249071	25.779444
187.001361	6326.971609	25.784461
187.132336	6329.654041	25.789479
187.385625	6325.920644	25.794496
187.242976	6342.484965	25.799514
187.658974	6353.230285	25.804532
187.912170	6341.059710	25.809549
187.953813	6355.331952	25.814567
188.243354	6346.914708	25.819584
188.076305	6358.784422	25.824602
188.608401	6373.759743	25.829620
188.689639	6378.281689	25.834637
188.901256	6388.675679	25.839655
189.415738	6391.131764	25.844672
188.963895	6412.966396	25.849690
189.128666	6415.913315	25.854708
189.663492	6410.829777	25.859725
189.454325	6435.045043	25.864743
189.860628	6439.658375	25.869760
190.083721	6447.373226	25.874778
190.441692	6452.919501	25.879796
190.660321	6473.525409	25.884813
190.481237	6464.412566	25.889831
191.105854	6472.792748	25.894848
191.122005	6493.829067	25.899866
191.241410	6489.540274	25.904884
191.512658	6488.017930	25.909901
191.646691	6489.751853	25.914919
191.928467	6498.012831	25.919936
191.935571	6521.729569	25.924954
191.982338	6502.506151	25.929972
192.380314	6523.424994	25.934989
192.218614	6536.984760	25.940007
193.045023	6542.315559	25.945024
193.183588	6545.763133	25.950042
193.306338	6549.889063	25.955060
193.727732	6556.164829	25.960077
193.518034	6562.793760	25.965095
193.727184	6573.261444	25.970112
193.835405	6571.217491	25.975130
193.657705	6579.606838	25.980148
194.117394	6597.712687	25.985165
194.112788	6603.633891	25.990183
194.761959	6617.727709	25.995200
194.886993	6631.875989	26.000218
195.104448	6643.243253	26.005236
195.191740	6636.148397	26.010253
195.187949	6657.989850	26.015271
195.712784	6657.053335	26.020288
195.900140	6662.559228	26.025306
196.074463	6686.585524	26.030324
196.197553	6687.750016	26.035341
196.002026	6704.763765	26.040359
196.461193	6704.065095	26.045376
196.789818	6713.662540	26.050394
196.813707	6727.880537	26.055412
197.439132	6726.504696	26.060429
197.314512	6747.598435	26.065447
197.441973	6750.720528	26.070464
197.472437	6770.906811	26.075482
197.802799	6780.326997	26.080500
198.136514	6783.443753	26.085517
198.357296	6798.357414	26.090535
198.942767	6801.157879	26.095552
198.904590	6810.149032	26.100570
198.922373	6807.881856	26.105588
198.986222	6820.378386	26.110605
199.469066	6827.941091	26.115623
199.621946	6841.572150	26.120640
199.492005	6856.020930	26.125658
199.790107	6870.209511	26.130676
200.064672	6874.718885	26.135693
200.159289	6885.941481	26.140711
200.420198	6895.209948	26.145728
201.017089	6906.456343	26.150746
200.863226	6915.480951	26.155764
201.283955	6921.576019	26.160781
201.177067	6928.054181	26.165799
201.317348	6928.915399	26.170816
201.583448	6958.510557	26.175834
201.813321	6951.081253	26.180852
202.047595	6954.141514	26.185869
201.923204	6981.011372	26.190887
202.394557	6970.460127	26.195904
202.600524	6972.292791	26.200922
202.792528	7011.213111	26.205940
203.231904	7007.449093	26.210957
203.348833	7017.959332	26.215975
203.359251	7018.273980	26.220992
203.681608	7030.043393	26.226010
204.007717	7039.805105	26.231028
204.396523	7033.007397	26.236045
203.949895	7052.990021	26.241063
204.249608	7056.175987	26.246080
204.638154	7070.608412	26.251098
204.578296	7090.388592	26.256116
205.113895	7094.035792	26.261133
205.456899	7095.361958	26.266151
205.525804	7097.752297	26.271168
205.742697	7112.450526	26.276186
205.945106	7123.358708	26.281204
206.256866	7115.651903	26.286221
206.404925	7141.503776	26.291239
206.660429	7143.050825	26.296256
207.127565	7145.043297	26.301274
206.758737	7157.435204	26.306292
207.297396	7157.684528	26.311309
207.268439	7185.794490	26.316327
207.517033	7174.527218	26.321344
207.800790	7192.096921	26.326362
207.935695	7210.918574	26.331380
208.581535	7199.528159	26.336397
208.200685	7217.873410	26.341415
208.825870	7224.299515	26.346432
209.274089	7235.355854	26.351450
209.043400	7229.630878	26.356468
209.457713	7245.488989	26.361485
209.589336	7250.902489	26.366503
209.962364	7258.231146	26.371520
210.218190	7248.270336	26.376538
209.924180	7264.945576	26.381556
210.540821	7264.720617	26.386573
210.398188	7292.254863	26.391591
210.533220	7287.602206	26.396608
210.682835	7304.977055	26.401626
210.968644	7315.771373	26.406644
211.082498	7317.470058	26.411661
211.083125	7346.101982	26.416679
211.494274	7348.381153	26.421696
211.840851	7366.381663	26.426714
211.769860	7378.512261	26.431732
212.411069	7391.327163	26.436749
212.645882	7405.856023	26.441767
213.002168	7411.602783	26.446784
212.841626	7409.888747	26.451802
212.890539	7416.837978	26.456820
213.339899	7435.992967	26.461837
213.321907	7441.360360	26.466855
213.712142	7454.501727	26.471872
213.972444	7465.959573	26.476890
213.598505	7475.034551	26.481908
214.612324	7473.617980	26.486925
214.405888	7492.411002	26.491943
214.617274	7497.093511	26.496960
214.851098	7505.774206	26.501978
214.939276	7519.417777	26.506996
215.321321	7536.396269	26.512013
215.718054	7544.603316	26.517031
215.809167	7553.800912	26.522048
216.235221	7558.031418	26.527066
215.843088	7578.731507	26.532084
216.423902	7582.580133	26.537101
216.878319	7598.994810	26.542119
217.113880	7602.599485	26.547136
217.571002	7591.632270	26.552154
217.400458	7617.320958	26.557172
217.926073	7621.470305	26.562189
218.071989	7637.108037	26.567207
218.152743	7647.294809	26.572224
218.365711	7634.881742	26.577242
218.219204	7668.274433	26.582260
218.882047	7658.165065	26.587277
219.177834	7663.675291	26.592295
219.103558	7685.682136	26.597312
219.613211	7699.316910	26.602330
219.604796	7702.429392	26.607348
220.070565	7709.015674	26.612365
220.271797	7715.615015	26.617383
220.092714	7722.368619	26.622400
220.545277	7725.679078	26.627418
220.476320	7740.849960	26.632436
221.137563	7754.020782	26.637453
221.018773	7763.799604	26.642471
221.167405	7780.230967	26.647488
221.623456	7779.488691	26.652506
221.628817	7800.951112	26.657524
221.953583	7805.463000	26.662541
222.243561	7816.109882	26.667559
222.355332	7827.107781	26.672576
222.593403	7835.504732	26.677594
222.688936	7851.495355	26.682612
223.092132	7852.397336	26.687629
223.507709	7868.862568	26.692647
223.827129	7866.774543	26.697664
224.009517	7889.675539	26.702682
224.003980	7893.330521	26.707700
224.331781	7907.962290	26.712717
224.140967	7903.064745	26.717735
224.698921	7924.447125	26.722752
225.137565	7921.905751	26.727770
224.983396	7937.479117	26.732788
225.310892	7940.320934	26.737805
225.768134	7948.827397	26.742823
225.589471	7958.611170	26.747840
225.942328	7958.575398	26.752858
225.878435	7978.328288	26.757876
226.143490	7980.171333	26.762893
226.258700	7998.221295	26.767911
226.631115	8017.586802	26.772928
227.115150	8010.021250	26.777946
227.148606	8025.689120	26.782964
227.695985	8044.727771	26.787981
227.826694	8045.426131	26.792999
227.536019	8047.183091	26.798016
228.042672	8066.641356	26.803034
228.300189	8082.364057	26.808052
228.534240	8096.868537	26.813069
228.837487	8105.820998	26.818087
229.118581	8114.016110	26.823104
229.568626	8129.770332	26.828122
229.285678	8135.750679	26.833140
229.407964	8154.116804	26.838157
230.025368	8161.458890	26.843175
230.073340	8172.294894	26.848192
230.594168	8193.581290	26.853210
231.225529	8194.494922	26.858228
231.126647	8188.806001	26.863245
231.197383	8206.829472	26.868263
231.247725	8221.431027	26.873280
231.741007	8224.396763	26.878298
231.792392	8234.967098	26.883316
232.071549	8243.656737	26.888333
232.194586	8255.986096	26.893351
232.296646	8259.648409	26.898368
232.427100	8279.126792	26.903386
232.660280	8298.641545	26.908404
232.896327	8302.779020	26.913421
233.581554	8327.514968	26.918439
233.584928	8345.861729	26.923456
233.982492	8336.961900	26.928474
233.906609	8363.843044	26.933492
234.141738	8370.602517	26.938509
234.627403	8381.447590	26.943527
234.398875	8409.152602	26.948544
234.872980	8404.418009	26.953562
234.865883	8430.048206	26.958580
235.261641	8443.505107	26.963597
235.879662	8460.987622	26.968615
236.027363	8476.405629	26.973632
236.448032	8480.318581	26.978650
236.280662	8496.260527	26.983668
236.887771	8509.445376	26.988685
237.226165	8501.949219	26.993703
237.358099	8526.550225	26.998720
237.846995	8525.165315	27.003738
237.819358	8526.752927	27.008756
237.978364	8529.950630	27.013773
238.502050	8532.247462	27.018791
238.413317	8554.077698	27.023808
238.374686	8556.387842	27.028826
238.575663	8553.609632	27.033844
238.464370	8571.620855	27.038861
239.179258	8579.657374	27.043879
239.354291	8612.513061	27.048896
239.783970	8616.275106	27.053914
239.682472	8621.894659	27.058932
240.240242	8637.532317	27.063949
240.555347	8646.947474	27.068967
240.968937	8650.575176	27.073984
241.015177	8659.140090	27.079002
241.109931	8664.076052	27.084020
241.677438	8668.646300	27.089037
241.846535	8685.984249	27.094055
241.815189	8702.996925	27.099072
242.048176	8700.764403	27.104090
242.379565	8718.614748	27.109108
242.448357	8718.754095	27.114125
242.850413	8727.607772	27.119143
243.003160	8745.202560	27.124160
243.247994	8754.444855	27.129178
243.662011	8764.794877	27.134196
243.930257	8783.926185	27.139213
244.111835	8784.808474	27.144231
244.535108	8804.431295	27.149248
244.616110	8805.688437	27.154266
244.704767	8807.606132	27.159284
245.322557	8818.152301	27.164301
245.418208	8841.348326	27.169319
245.303722	8845.799535	27.174336
246.045021	8858.011956	27.179354
245.868588	8857.019500	27.184372
245.918619	8889.265816	27.189389
246.334484	8888.248193	27.194407
246.449444	8921.419450	27.199424
246.729063	8936.814152	27.204442
246.733422	8941.410119	27.209460
247.246305	8955.224951	27.214477
248.051464	8966.323663	27.219495
247.785636	9008.826628	27.224512
248.169762	8992.155185	27.229530
248.583145	9013.298176	27.234548
249.040279	9011.062144	27.239565
249.596214	9028.316010	27.244583
249.784736	9033.403185	27.249600
249.770795	9053.467836	27.254618
250.053909	9059.898919	27.259636
249.901976	9043.844416	27.264653
250.480088	9067.961679	27.269671
250.116619	9083.082112	27.274688
250.442487	9083.582986	27.279706
250.861644	9097.214985	27.284724
250.986694	9118.784160	27.289741
251.305973	9113.335125	27.294759
251.437727	9137.006651	27.299776
251.676168	9131.441049	27.304794
251.897724	9155.136455	27.309812
252.256892	9167.717725	27.314829
252.231505	9181.830638	27.319847
252.205152	9197.405793	27.324864
252.876108	9223.083505	27.329882
253.402353	9231.403837	27.334900
253.242654	9241.821640	27.339917
253.660682	9257.178873	27.344935
253.793753	9280.085932	27.349952
254.378623	9282.955450	27.354970
254.492194	9310.887741	27.359988
254.736996	9325.117859	27.365005
255.264956	9321.043278	27.370023
255.208697	9348.827622	27.375040
255.863237	9358.941812	27.380058
256.191639	9362.983812	27.385076
256.340813	9384.791109	27.390093
256.701042	9389.653520	27.395111
256.811444	9406.453574	27.400128
257.033269	9406.461908	27.405146
257.206024	9415.837289	27.410164
257.427835	9423.222605	27.415181
257.487776	9441.690356	27.420199
257.379387	9451.599644	27.425216
258.168546	9479.681496	27.430234
258.537634	9483.390471	27.435252
258.635127	9507.491016	27.440269
258.809391	9519.488648	27.445287
258.976280	9534.077238	27.450304
259.246090	9538.628323	27.455322
259.333892	9567.604731	27.460340
259.488006	9589.290351	27.465357
260.165431	9607.677983	27.470375
260.366231	9619.933120	27.475392
260.575990	9632.103031	27.480410
261.119628	9648.449098	27.485428
261.213367	9667.205265	27.490445
261.594235	9662.888056	27.495463
261.786223	9687.272076	27.500480
261.938722	9697.922155	27.505498
262.439257	9715.828182	27.510516
262.516855	9734.520510	27.515533
262.609451	9741.524455	27.520551
262.951738	9757.658392	27.525568
262.977959	9781.856122	27.530586
263.248612	9791.272794	27.535604
263.445109	9811.282882	27.540621
264.106972	9820.176070	27.545639
264.284966	9842.472459	27.550656
264.558966	9857.859170	27.555674
264.942994	9852.446373	27.560692
265.064245	9878.569712	27.565709
265.715699	9875.045836	27.570727
265.748014	9890.010347	27.575744
265.682864	9905.513334	27.580762
266.317520	9918.861881	27.585780
266.355428	9924.127609	27.590797
266.559940	9945.486606	27.595815
266.579934	9959.502911	27.600832
267.058946	9981.845175	27.605850
267.492977	9984.060526	27.610868
267.301854	10012.637625	27.615885
267.851596	10022.231879	27.620903
268.132569	10043.004353	27.625920
267.943500	10062.337283	27.630938
268.788826	10058.145033	27.635956
269.302685	10081.654059	27.640973
269.796900	10094.464838	27.645991
270.076381	10100.340181	27.651008
270.327640	10098.702238	27.656026
270.526463	10102.942160	27.661044
270.641050	10119.551509	27.666061
270.992440	10118.248980	27.671079
271.508280	10146.127368	27.676096
271.508417	10146.086836	27.681114
271.924280	10143.971725	27.686132
271.812225	10170.454624	27.691149
272.294695	10165.517089	27.696167
272.550220	10186.849805	27.701184
272.692861	10206.326790	27.706202
272.791802	10209.859446	27.711220
272.988758	10235.326818	27.716237
273.384369	10240.605290	27.721255
273.849620	10266.671327	27.726272
273.853497	10268.320991	27.731290
274.541197	10284.746708	27.736308
274.688888	10296.575673	27.741325
274.846326	10305.897786	27.746343
275.200912	10334.104028	27.751360
275.294682	10335.665003	27.756378
275.986958	10357.431223	27.761396
275.886123	10368.135535	27.766413
276.548425	10375.237060	27.771431
276.786829	10391.868685	27.776448
276.911216	10404.676113	27.781466
277.336647	10417.518989	27.786484
277.608727	10423.596711	27.791501
277.860798	10430.559822	27.796519
278.099578	10447.853687	27.801536
278.417869	10453.812306	27.806554
278.420486	10457.372571	27.811572
278.362643	10485.094737	27.816589
278.985538	10493.060797	27.821607
279.341525	10504.448680	27.826624
279.204855	10516.715055	27.831642
279.614607	10530.028385	27.836660
279.796619	10547.498646	27.841677
279.968018	10551.620299	27.846695
280.319600	10579.494982	27.851712
280.463809	10585.573477	27.856730
280.939915	10605.043082	27.861748
280.815309	10623.554685	27.866765
281.502252	10641.185000	27.871783
281.874480	10652.500759	27.876800
282.069535	10675.967487	27.881818
282.560641	10682.528243	27.886836
282.762457	10709.241837	27.891853
282.907522	10710.348454	27.896871
283.174550	10725.324394	27.901888
283.799371	10742.671971	27.906906
284.019051	10755.811966	27.911924
284.195606	10765.619252	27.916941
284.621095	10793.128014	27.921959
285.233668	10793.481344	27.926976
284.970247	10802.799621	27.931994
285.449838	10819.468044	27.937012
285.519812	10830.114768	27.942029
286.033610	10859.953244	27.947047
286.201549	10854.613098	27.952064
286.422456	10886.747935	27.957082
287.017791	10880.120209	27.962100
287.282318	10895.220276	27.967117
287.450799	10917.267938	27.972135
287.948149	10921.758000	27.977152
288.099230	10943.191074	27.982170
288.607577	10951.872527	27.987188
288.495195	10960.435311	27.992205
288.722717	10970.290092	27.997223
288.905088	10984.785940	28.002240
288.863956	11010.483815	28.007258
289.396032	11015.101767	28.012276
289.545667	11042.407439	28.017293
290.031294	11074.483171	28.022311
290.516066	11083.330582	28.027328
290.513317	11095.022029	28.032346
290.890835	11119.212354	28.037364
291.291188	11127.201633	28.042381
291.761985	11141.287671	28.047399
291.895256	11161.505996	28.052416
291.927717	11184.846358	28.057434
292.675047	11180.978335	28.062452
292.617130	11219.843596	28.067469
293.058657	11226.775309	28.072487
293.514253	11241.828154	28.077504
293.676791	11259.402691	28.082522
294.280665	11276.681034	28.087540
294.485736	11293.587344	28.092557
294.592941	11298.116091	28.097575
294.709345	11315.688209	28.102592
294.634635	11341.976360	28.107610
295.371109	11343.542436	28.112628
295.283676	11359.674577	28.117645
295.321827	11384.207858	28.122663
296.225702	11399.504422	28.127680
296.221133	11417.631901	28.132698
296.770142	11434.660634	28.137716
296.911851	11450.688274	28.142733
297.322696	11461.205561	28.147751
297.399357	11488.714132	28.152768
297.929882	11495.735674	28.157786
298.337094	11516.669510	28.162804
298.429734	11524.874108	28.167821
298.555512	11551.552125	28.172839
299.154683	11569.859026	28.177856
299.152431	11590.609915	28.182874
299.776816	11602.605554	28.187892
299.947678	11621.074043	28.192909
300.272083	11630.118123	28.197927
300.866206	11634.009393	28.202944
300.832591	11676.524195	28.207962
301.516106	11673.757844	28.212980
301.652171	11687.307072	28.217997
301.981321	11706.338356	28.223015
302.804263	11710.645727	28.228032
302.506428	11734.032102	28.233050
302.864091	11739.301416	28.238068
303.013846	11771.358182	28.243085
303.367745	11776.200352	28.248103
304.205660	11792.177212	28.253120
303.967329	11803.897309	28.258138
304.574391	11823.779713	28.263156
304.686065	11838.721313	28.268173
304.589364	11856.621986	28.273191
305.093947	11871.105507	28.278208
305.264808	11879.773602	28.283226
305.669852	11905.255891	28.288244
306.259402	11914.887526	28.293261
306.542129	11949.082749	28.298279
306.983105	11964.283270	28.303296
307.025266	11979.069233	28.308314
307.702182	11993.711546	28.313332
307.717252	12012.747624	28.318349
307.778899	12020.087734	28.323367
308.415156	12041.144782	28.328384
308.424983	12055.860022	28.333402
308.689132	12071.603175	28.338420
309.317146	12091.664405	28.343437
309.665877	12109.270861	28.348455
310.166092	12116.913009	28.353472
310.069242	12131.352930	28.358490
310.547885	12142.244764	28.363508
310.811608	12154.959655	28.368525
310.978634	12180.488410	28.373543
311.791904	12193.404801	28.378560
311.639056	12193.336698	28.383578
312.015591	12210.529568	28.388596
312.245486	12221.759794	28.393613
312.333754	12236.605364	28.398631
312.917820	12248.461160	28.403648
312.788284	12275.625444	28.408666
313.564915	12285.195627	28.413684
313.954945	12306.482956	28.418701
314.040268	12329.471334	28.423719
314.344497	12332.343099	28.428736
314.573600	12349.686736	28.433754
314.934749	12365.671914	28.438772
315.220393	12389.345481	28.443789
315.737419	12392.401365	28.448807
316.326659	12419.747297	28.453824
316.002169	12438.089711	28.458842
316.414542	12451.294927	28.463860
316.828631	12471.713853	28.468877
317.425102	12490.564211	28.473895
317.676024	12507.978144	28.478912
318.083891	12523.110128	28.483930
318.551552	12531.061491	28.488948
318.762080	12547.121829	28.493965
318.720062	12549.620645	28.498983
319.339510	12571.697830	28.504000
318.966044	12595.542876	28.509018
319.735930	12611.710516	28.514036
319.795138	12638.700743	28.519053
319.948333	12652.086360	28.524071
320.528731	12679.366482	28.529088
320.475833	12695.897136	28.534106
321.007549	12738.060357	28.539124
321.628071	12749.942223	28.544141
321.824443	12772.739037	28.549159
322.479863	12778.363472	28.554176
322.973874	12811.429172	28.559194
323.075549	12817.012196	28.564212
323.539497	12834.296924	28.569229
323.693885	12848.335029	28.574247
324.014823	12868.859459	28.579264
324.539156	12891.566208	28.584282
324.761393	12910.755760	28.589300
324.648497	12934.772328	28.594317
325.105929	12949.670942	28.599335
325.627409	12961.987500	28.604352
325.605594	12979.261258	28.609370
326.169773	13001.713294	28.614388
326.359918	13016.783263	28.619405
326.635025	13035.607987	28.624423
327.241444	13071.352777	28.629440
327.260360	13082.114303	28.634458
327.790341	13098.738263	28.639476
328.091491	13127.179425	28.644493
328.305559	13134.221476	28.649511
329.020609	13155.047724	28.654528
329.317255	13171.916551	28.659546
329.610871	13177.429174	28.664564
330.053462	13197.667241	28.669581
330.303799	13201.284505	28.674599
330.635885	13228.252364	28.679616
330.886704	13232.368593	28.684634
331.028595	13246.954925	28.689652
331.397291	13257.711405	28.694669
331.199618	13287.495493	28.699687
331.741807	13299.140761	28.704704
332.193494	13327.690939	28.709722
332.393382	13353.774110	28.714740
332.956760	13360.313119	28.719757
332.836637	13389.137742	28.724775
333.320201	13409.878243	28.729792
333.729424	13426.716229	28.734810
334.039069	13457.029235	28.739828
334.748575	13474.038242	28.744845
334.695519	13490.800611	28.749863
335.242466	13514.889257	28.754880
335.600293	13537.225810	28.759898
335.892124	13555.279485	28.764916
336.362854	13586.898125	28.769933
336.790880	13596.116181	28.774951
336.887422	13619.308985	28.779968
337.467630	13627.368149	28.784986
337.370355	13655.920827	28.790004
338.109374	13667.499788	28.795021
338.175115	13703.011666	28.800039
338.940176	13714.400158	28.805056
339.115444	13727.504262	28.810074
339.515624	13751.936845	28.815092
339.805871	13766.271073	28.820109
340.001264	13793.050369	28.825127
340.359584	13807.301271	28.830144
340.643714	13833.359048	28.835162
340.891676	13844.288287	28.840180
341.433921	13877.996056	28.845197
341.577412	13890.177411	28.850215
342.141159	13918.302212	28.855232
342.682990	13941.604509	28.860250
342.686215	13949.154210	28.865268
343.123159	13974.339224	28.870285
343.680819	13994.521447	28.875303
343.944920	14021.493971	28.880320
344.088680	14027.137742	28.885338
344.818766	14055.992160	28.890356
345.317910	14061.787023	28.895373
345.205925	14088.080945	28.900391
345.583745	14102.254040	28.905408
345.784263	14128.645259	28.910426
346.200107	14149.007818	28.915444
346.439118	14171.061868	28.920461
346.962599	14186.615841	28.925479
347.230020	14201.206403	28.930496
347.497295	14218.473773	28.935514
347.958607	14236.208914	28.940532
348.240665	14249.483600	28.945549
348.146693	14276.701771	28.950567
348.493709	14284.803960	28.955584
348.821583	14312.093315	28.960602
349.162280	14338.361088	28.965620
349.585167	14362.794477	28.970637
350.087675	14383.150722	28.975655
350.653059	14400.266492	28.980672
350.603119	14436.839064	28.985690
351.211573	14451.274369	28.990708
351.633007	14471.785148	28.995725
351.708711	14495.896819	29.000743
352.318916	14515.050875	29.005760
352.807658	14544.012279	29.010778
353.068561	14551.321173	29.015796
353.507596	14580.754320	29.020813
353.344484	14594.935651	29.025831
354.143715	14627.082787	29.030848
354.427760	14648.411843	29.035866
354.430728	14678.438445	29.040884
355.208316	14686.946322	29.045901
355.685938	14715.597014	29.050919
356.327639	14721.414679	29.055936
356.868100	14732.162647	29.060954
357.212758	14756.142720	29.065972
357.654044	14755.194890	29.070989
357.972214	14769.003407	29.076007
358.548878	14782.579850	29.081024
358.748992	14794.891452	29.086042
358.742212	14807.785007	29.091060
359.472144	14818.598588	29.096077
359.406776	14840.504915	29.101095
359.417044	14859.472009	29.106112
359.944107	14877.042440	29.111130
360.217588	14911.944250	29.116148
360.688933	14912.094988	29.121165
361.163908	14949.695074	29.126183
361.424665	14948.661659	29.131200
361.843287	14988.209637	29.136218
362.095604	15003.648445	29.141236
362.508911	15023.030731	29.146253
362.632488	15043.334885	29.151271
363.036977	15065.036870	29.156288
363.488741	15093.644766	29.161306
363.317732	15112.410209	29.166324
363.647601	15137.964717	29.171341
364.167992	15181.623765	29.176359
364.726178	15202.378932	29.181376
365.031182	15217.758293	29.186394
365.434833	15253.013576	29.191412
365.871993	15270.630374	29.196429
366.393440	15286.933267	29.201447
366.474187	15309.556185	29.206464
367.087040	15338.305073	29.211482
367.406088	15364.318571	29.216500
367.713973	15369.207516	29.221517
367.776231	15392.848536	29.226535
368.552000	15403.010097	29.231552
368.509573	15435.555794	29.236570
368.999238	15447.264325	29.241588
369.494991	15477.975419	29.246605
369.790487	15504.097413	29.251623
369.822552	15528.082356	29.256640
370.554801	15546.526678	29.261658
370.949852	15572.750421	29.266676
371.366284	15587.443442	29.271693
371.748920	15625.118969	29.276711
372.421048	15637.726041	29.281728
372.582554	15663.163894	29.286746
372.794944	15685.135905	29.291764
373.419918	15702.930123	29.296781
373.679481	15723.378732	29.301799
374.002509	15739.706741	29.306816
374.538291	15767.477081	29.311834
374.611984	15781.160837	29.316852
374.983903	15813.001177	29.321869
375.024406	15835.249662	29.326887
375.363658	15861.364111	29.331904
376.071750	15895.595183	29.336922
376.333344	15921.565741	29.341940
376.953675	15952.557980	29.346957
377.469212	15970.522874	29.351975
377.881435	15991.625444	29.356992
378.590458	16010.969932	29.362010
379.060245	16027.084050	29.367028
379.540184	16042.545992	29.372045
379.520266	16064.302851	29.377063
379.953781	16080.154642	29.382080
380.471125	16092.946079	29.387098
380.606833	16130.489389	29.392116
381.160304	16143.773944	29.397133
381.354236	16161.826425	29.402151
381.605142	16177.008220	29.407168
382.010053	16204.301963	29.412186
382.534842	16226.688477	29.417204
382.854055	16253.742657	29.422221
382.913491	16281.672397	29.427239
383.263708	16293.661336	29.432256
383.723690	16323.431355	29.437274
383.785488	16349.011014	29.442292
384.327184	16386.293733	29.447309
385.063693	16400.866467	29.452327
385.350549	16427.863915	29.457344
385.774024	16461.412481	29.462362
386.161139	16481.325809	29.467380
386.919050	16491.716309	29.472397
387.434667	16524.350266	29.477415
387.516542	16531.786358	29.482432
388.011120	16530.027301	29.487450
388.290559	16563.363444	29.492468
388.613372	16581.302981	29.497485
388.819937	16585.142374	29.502503
388.866174	16617.122681	29.507520
389.724586	16644.633882	29.512538
389.608185	16670.204679	29.517556
390.330567	16689.045308	29.522573
390.517273	16713.160588	29.527591
390.873469	16739.441328	29.532608
391.524368	16762.276186	29.537626
391.826879	16792.578242	29.542644
392.487880	16793.979045	29.547661
392.980012	16822.955246	29.552679
393.122852	16843.579732	29.557696
393.831752	16860.786705	29.562714
393.788556	16889.581826	29.567732
394.297101	16904.745630	29.572749
394.701454	16925.583842	29.577767
394.792907	16965.155387	29.582784
395.686452	16981.228479	29.587802
395.522503	17007.646289	29.592820
395.816125	17034.248689	29.597837
396.619567	17062.885220	29.602855
396.740428	17091.042439	29.607872
397.266824	17111.089493	29.612890
397.598854	17144.557869	29.617908
398.285697	17169.447036	29.622925
398.856354	17191.177322	29.627943
399.198800	17223.599238	29.632960
399.887870	17238.990291	29.637978
399.822953	17274.917238	29.642996
400.176560	17280.614299	29.648013
400.594069	17314.689050	29.653031
400.847578	17337.033211	29.658048
401.185718	17373.533508	29.663066
401.393008	17392.262408	29.668084
402.134539	17410.425147	29.673101
402.392966	17448.644473	29.678119
402.818296	17475.790577	29.683136
403.593805	17509.994136	29.688154
403.940195	17531.550417	29.693172
404.416223	17551.856445	29.698189
404.932332	17576.492198	29.703207
404.828672	17602.380787	29.708224
405.472248	17614.326576	29.713242
405.961612	17653.713855	29.718260
406.243020	17665.720145	29.723277
406.742688	17690.727374	29.728295
407.062473	17732.969238	29.733312
407.490953	17751.684393	29.738330
408.085006	17776.082666	29.743348
408.497024	17807.472150	29.748365
408.885274	17825.773555	29.753383
408.975067	17839.647801	29.758400
409.548352	17862.381510	29.763418
409.953419	17889.578418	29.768436
410.548955	17899.473539	29.773453
410.682792	17919.040522	29.778471
411.011491	17939.200072	29.783488
411.672378	17951.971276	29.788506
411.792768	17987.003857	29.793524
411.846476	18005.226698	29.798541
412.461576	18030.912116	29.803559
413.019828	18071.536669	29.808576
413.376373	18097.388585	29.813594
413.424456	18124.134931	29.818612
414.026797	18143.385829	29.823629
414.242048	18184.457832	29.828647
414.518918	18221.781280	29.833664
415.171906	18234.272885	29.838682
415.427868	18282.408892	29.843700
415.633381	18318.599490	29.848717
416.435782	18337.958515	29.853735
416.483882	18380.641090	29.858752
417.280706	18423.189135	29.863770
417.588123	18442.475585	29.868788
418.282940	18471.407628	29.873805
419.321954	18494.435775	29.878823
419.579057	18526.125409	29.883840
420.303801	18542.877421	29.888858
420.632980	18561.121196	29.893876
420.757360	18587.669179	29.898893
421.597742	18604.774878	29.903911
421.720160	18636.752729	29.908928
422.111255	18643.441168	29.913946
422.227824	18680.598742	29.918964
422.785451	18701.367688	29.923981
423.197121	18723.538260	29.928999
423.491774	18773.234975	29.934016
423.904380	18787.852732	29.939034
424.487369	18810.719757	29.944052
425.070448	18851.869173	29.949069
425.607767	18856.775737	29.954087
426.236348	18896.513685	29.959104
426.366457	18903.340669	29.964122
426.659128	18941.320422	29.969140
426.864401	18969.310122	29.974157
427.466933	18978.548125	29.979175
427.440278	19011.735554	29.984192
427.928489	19035.817636	29.989210
428.518636	19078.560256	29.994228
429.242905	19109.614435	29.999245
429.666085	19125.427703	30.004263
429.924856	19161.991710	30.009280
430.648125	19189.662658	30.014298
431.041874	19214.471505	30.019316
431.729418	19242.260841	30.024333
431.978416	19256.807073	30.029351
431.937662	19284.345576	30.034368
432.566571	19294.170926	30.039386
432.886085	19328.335407	30.044404
432.990916	19358.739928	30.049421
433.842034	19387.942102	30.054439
433.600714	19407.519153	30.059456
434.066025	19443.007170	30.064474
434.528134	19479.665910	30.069492
435.050616	19502.203422	30.074509
435.721385	19544.393114	30.079527
436.003999	19566.951612	30.084544
436.515534	19590.123312	30.089562
437.534093	19612.448084	30.094580
437.665318	19636.020619	30.099597
438.207545	19660.583675	30.104615
438.493367	19697.934833	30.109632
439.228264	19711.747740	30.114650
439.421751	19744.121685	30.119668
439.424645	19769.372451	30.124685
440.182746	19795.920356	30.129703
440.294287	19827.220843	30.134720
440.918420	19860.306787	30.139738
441.624692	19895.410572	30.144756
441.823150	19934.992911	30.149773
442.433579	19967.981654	30.154791
442.753057	20001.012095	30.159808
443.240517	20021.412464	30.164826
443.503234	20064.321382	30.169844
443.935154	20090.294932	30.174861
444.853184	20120.141029	30.179879
444.798359	20145.665794	30.184896
445.127163	20182.994334	30.189914
446.011725	20207.080447	30.194932
446.113826	20241.642229	30.199949
447.127668	20276.144670	30.204967
447.042614	20315.546740	30.209984
448.057644	20329.840820	30.215002
448.152267	20368.368644	30.220020
448.279347	20404.380106	30.225037
449.330226	20433.136629	30.230055
449.216746	20457.894786	30.235072
449.821304	20494.922237	30.240090
450.292316	20529.234129	30.245108
450.840532	20563.225886	30.250125
451.498926	20594.827053	30.255143
452.284146	20631.970159	30.260160
452.573362	20654.407509	30.265178
453.229929	20677.739634	30.270196
453.220807	20696.640672	30.275213
454.007943	20722.301566	30.280231
454.477881	20752.126155	30.285248
454.592903	20781.858900	30.290266
455.190946	20805.465141	30.295284
455.325623	20834.889697	30.300301
456.259316	20848.498699	30.305319
456.294508	20896.038883	30.310336
456.789589	20922.164801	30.315354
456.886131	20938.150077	30.320372
457.190246	20982.237365	30.325389
457.966966	21005.297653	30.330407
458.273897	21036.526510	30.335424
459.020969	21072.591544	30.340442
459.531889	21101.750726	30.345460
459.855693	21123.385482	30.350477
460.548400	21148.507313	30.355495
460.948788	21187.962210	30.360512
461.523497	21200.305672	30.365530
461.939276	21226.271082	30.370548
461.890695	21258.292565	30.375565
462.691402	21285.578862	30.380583
462.823367	21321.582594	30.385600
463.465598	21355.665445	30.390618
464.117431	21386.256492	30.395636
464.417158	21421.056364	30.400653
465.099025	21450.359857	30.405671
465.135037	21483.156646	30.410688
465.582926	21510.839758	30.415706
466.374878	21547.742193	30.420724
466.692939	21586.701669	30.425741
467.223466	21603.396579	30.430759
467.592464	21652.375907	30.435776
467.737102	21676.554998	30.440794
468.391476	21722.979956	30.445812
469.141307	21761.098494	30.450829
469.352963	21795.495035	30.455847
470.147405	21817.609817	30.460864
470.654317	21854.140191	30.465882
471.123577	21891.229513	30.470900
471.194798	21928.405172	30.475917
472.238026	21950.623059	30.480935
472.717361	21988.422174	30.485952
472.607936	22032.799986	30.490970
473.427588	22049.909252	30.495988
474.074367	22082.098072	30.501005
474.515652	22117.380191	30.506023
475.180535	22149.165391	30.511040
475.587231	22176.682187	30.516058
475.978897	22206.093966	30.521076
476.099304	22254.720981	30.526093
476.740230	22285.974723	30.531111
477.328104	22317.781195	30.536128
477.662653	22337.945895	30.541146
478.177148	22377.772303	30.546164
478.537628	22417.603658	30.551181
479.201191	22436.683548	30.556199
479.535752	22476.487676	30.561216
480.457080	22511.559529	30.566234
481.136594	22538.420753	30.571252
480.954540	22572.470585	30.576269
481.286345	22598.034216	30.581287
482.156907	22620.383737	30.586304
482.798906	22657.427658	30.591322
482.923465	22686.266195	30.596340
483.245636	22716.609913	30.601357
483.958112	22747.593266	30.606375
484.062514	22771.355929	30.611392
484.719720	22801.341637	30.616410
485.262297	22839.198090	30.621428
485.565380	22880.048678	30.626445
485.974189	22903.186519	30.631463
486.311192	22927.038381	30.636480
486.850820	22954.634599	30.641498
487.458688	23002.895636	30.646516
487.654622	23037.827454	30.651533
488.365198	23070.501182	30.656551
488.908436	23119.663666	30.661568
489.361885	23159.934965	30.666586
490.292006	23184.251157	30.671604
490.497838	23233.673314	30.676621
491.005320	23260.870348	30.681639
491.940771	23293.098362	30.686656
492.483009	23332.745545	30.691674
492.555010	23361.392839	30.696692
493.092710	23389.494209	30.701709
493.960331	23426.250377	30.706727
494.188810	23454.881578	30.711744
494.688170	23488.266396	30.716762
495.159411	23520.038740	30.721780
495.290169	23554.246424	30.726797
496.178069	23588.552538	30.731815
497.113976	23612.775531	30.736832
497.093322	23657.749454	30.741850
497.920455	23693.246158	30.746868
498.260783	23723.165160	30.751885
498.682687	23747.408800	30.756903
499.060704	23784.102803	30.761920
499.755179	23826.530230	30.766938
500.614221	23859.158311	30.771956
500.837057	23880.388785	30.776973
501.351207	23911.059447	30.781991
501.689477	23951.481070	30.787008
502.403631	23989.911572	30.792026
502.846867	24012.567442	30.797044
503.275879	24045.720466	30.802061
503.936953	24074.914011	30.807079
504.323506	24096.241572	30.812096
504.554608	24140.582857	30.817114
505.418548	24174.438787	30.822132
505.865017	24205.724945	30.827149
506.339656	24244.699116	30.832167
506.625523	24284.689624	30.837184
507.216046	24323.757380	30.842202
507.823684	24339.353554	30.847220
508.248231	24384.212143	30.852237
508.839340	24419.945782	30.857255
509.352195	24447.716648	30.862272
509.206672	24489.015415	30.867290
510.096116	24511.303965	30.872308
510.406402	24552.394809	30.877325
511.110396	24582.953823	30.882343
511.275596	24616.602984	30.887360
511.726712	24659.308500	30.892378
512.075575	24688.638765	30.897396
512.552018	24735.972902	30.902413
513.089206	24773.583562	30.907431
513.465691	24804.067563	30.912448
513.933003	24856.644891	30.917466
514.692193	24894.516653	30.922484
515.102473	24943.828852	30.927501
515.839294	24976.290441	30.932519
516.845149	25012.698224	30.937536
517.113997	25060.086871	30.942554
517.905159	25088.859039	30.947572
518.224427	25138.486458	30.952589
518.852316	25167.710145	30.957607
519.341396	25195.937469	30.962624
519.567939	25243.546873	30.967642
520.306303	25267.567553	30.972660
520.746704	25314.274242	30.977677
521.548645	25353.779551	30.982695
522.194004	25390.958519	30.987712
522.603968	25418.675786	30.992730
523.117553	25446.656243	30.997748
523.513765	25490.299107	31.002765
524.294519	25528.759747	31.007783
524.922239	25552.143084	31.012800
524.956187	25591.793368	31.017818
525.923687	25627.450075	31.022836
526.563445	25658.406596	31.027853
526.822504	25693.631960	31.032871
527.452902	25736.319682	31.037888
527.706866	25768.209905	31.042906
528.269036	25800.014863	31.047924
528.716352	25846.117800	31.052941
529.385423	25876.914889	31.057959
529.996049	25911.492343	31.062976
530.650176	25963.713491	31.067994
531.138062	25991.364987	31.073012
531.699952	26026.074918	31.078029
531.954609	26060.614074	31.083047
532.855462	26101.495100	31.088064
533.376848	26131.236963	31.093082
533.954345	26170.575226	31.098100
534.080165	26206.191617	31.103117
534.621161	26241.862488	31.108135
535.489166	26268.647239	31.113152
535.831947	26326.956675	31.118170
536.491456	26341.581531	31.123188
536.954623	26379.688314	31.128205
537.258742	26426.544427	31.133223
537.648705	26453.923991	31.138240
538.035162	26484.159096	31.143258
538.748434	26514.415469	31.148276
539.226438	26562.002133	31.153293
539.532265	26600.135289	31.158311
540.061175	26617.291104	31.163328
540.652747	26673.446162	31.168346
541.279157	26708.768868	31.173364
542.100067	26740.623509	31.178381
542.325168	26783.115453	31.183399
542.965877	26823.819965	31.188416
543.371621	26862.951733	31.193434
544.112732	26902.684847	31.198452
544.563593	26936.133463	31.203469
545.018711	26977.879471	31.208487
545.618074	27022.266207	31.213504
546.212149	27073.441718	31.218522
546.661278	27100.923257	31.223540
547.185329	27150.063418	31.228557
547.421356	27191.992200	31.233575
548.264859	27231.459294	31.238592
548.662443	27285.439122	31.243610
549.394001	27316.346417	31.248628
550.179817	27364.590751	31.253645
550.612515	27407.158424	31.258663
551.264415	27448.177081	31.263680
551.461775	27494.633396	31.268698
552.619873	27536.754986	31.273716
552.929600	27577.633876	31.278733
553.461308	27611.527179	31.283751
554.074859	27651.685051	31.288768
554.501609	27697.143458	31.293786
555.745448	27733.519548	31.298804
556.292228	27776.548251	31.303821
556.330295	27813.665696	31.308839
557.207148	27856.768099	31.313856
557.486702	27885.622065	31.318874
558.454327	27921.472956	31.323892
559.124406	27966.964276	31.328909
559.778609	27987.355461	31.333927
560.369795	28015.975668	31.338944
560.856424	28057.999939	31.343962
561.786626	28075.622848	31.348980
561.965666	28116.681492	31.353997
562.669400	28154.223147	31.359015
563.209293	28177.008987	31.364032
563.653151	28218.717462	31.369050
564.054218	28236.773061	31.374068
564.406262	28283.634825	31.379085
564.701336	28322.182678	31.384103
565.335815	28366.358741	31.389120
565.726191	28407.995858	31.394138
566.344859	28439.264445	31.399156
566.993605	28486.418332	31.404173
567.282732	28535.214857	31.409191
568.133397	28561.577597	31.414208
568.756010	28595.490009	31.419226
569.291303	28644.950457	31.424244
569.966806	28674.937216	31.429261
570.300775	28703.738280	31.434279
570.863968	28744.119625	31.439296
571.021917	28785.200657	31.444314
571.762049	28811.920208	31.449332
572.381562	28864.078287	31.454349
572.623983	28913.603533	31.459367
573.279037	28957.395013	31.464384
573.709118	28999.139211	31.469402
574.381416	29056.144594	31.474420
575.283117	29092.520735	31.479437
575.472508	29152.343727	31.484455
576.377924	29183.103216	31.489472
576.594895	29239.245713	31.494490
577.582685	29274.267512	31.499508
578.158924	29317.059249	31.504525
578.596385	29373.461779	31.509543
579.431169	29406.793705	31.514560
579.900680	29451.517460	31.519578
580.329954	29495.748197	31.524596
581.199606	29534.040384	31.529613
581.785429	29594.296691	31.534631
582.534620	29628.282510	31.539648
582.737949	29684.217549	31.544666
583.659646	29722.347456	31.549684
584.210405	29758.308218	31.554701
584.540664	29819.832104	31.559719
585.147439	29852.054006	31.564736
585.555081	29915.568898	31.569754
586.537859	29948.460755	31.574772
587.021803	29992.253914	31.579789
587.585997	30036.154180	31.584807
588.287090	30080.377889	31.589824
588.868801	30133.395490	31.594842
589.480906	30176.013578	31.599860
590.183611	30206.747412	31.604877
590.575094	30266.499764	31.609895
591.096256	30310.473813	31.614912
591.892658	30351.688789	31.619930
592.746823	30406.192557	31.624948
593.474461	30453.267105	31.629965
593.505364	30479.141022	31.634983
594.189635	30534.152943	31.640000
594.636426	30582.654712	31.645018
595.190614	30622.101308	31.650036
596.160009	30663.090951	31.655053
596.720642	30718.597553	31.660071
597.222333	30755.233398	31.665088
597.885106	30799.822914	31.670106
598.286640	30845.614087	31.675124
598.992778	30887.205696	31.680141
599.273590	30938.888531	31.685159
600.134164	30975.155669	31.690176
600.656594	31022.187314	31.695194
601.003305	31057.627109	31.700212
601.630323	31097.413132	31.705229
602.009255	31143.046407	31.710247
602.775994	31177.678842	31.715264
603.709143	31229.417889	31.720282
604.258873	31276.909273	31.725300
604.955333	31312.315988	31.730317
605.113861	31359.970778	31.735335
606.006059	31401.248804	31.740352
606.451273	31447.290026	31.745370
606.972647	31499.651850	31.750388
608.054479	31529.019677	31.755405
608.067172	31588.640175	31.760423
609.104108	31618.425090	31.765440
609.709178	31678.003590	31.770458
610.364612	31712.914938	31.775476
610.900018	31769.861781	31.780493
611.094481	31807.344832	31.785511
611.803083	31862.525991	31.790528
612.077836	31904.995847	31.795546
612.564734	31969.059306	31.800564
613.706490	32012.212523	31.805581
614.123893	32084.451738	31.810599
615.005146	32120.279967	31.815616
615.650644	32185.042450	31.820634
616.568531	32225.628124	31.825652
617.281640	32264.192808	31.830669
618.045863	32302.779391	31.835687
618.798175	32348.354987	31.840704
619.592819	32391.274470	31.845722
619.776357	32435.495557	31.850740
620.740768	32473.262589	31.855757
620.896429	32530.215799	31.860775
621.508876	32565.181517	31.865792
622.281412	32613.344260	31.870810
623.036493	32660.910979	31.875828
623.766948	32697.842585	31.880845
624.182749	32749.202270	31.885863
624.691560	32789.975849	31.890880
625.712588	32831.777598	31.895898
626.055734	32877.648365	31.900916
626.876490	32908.125753	31.905933
627.266880	32970.952257	31.910951
627.819469	33009.356685	31.915968
628.578798	33040.701556	31.920986
629.206428	33106.824474	31.926004
629.668937	33142.776787	31.931021
630.291940	33192.557015	31.936039
630.818169	33248.786956	31.941056
631.297796	33295.702681	31.946074
631.782919	33360.117030	31.951092
632.886106	33393.113305	31.956109
633.276108	33444.261741	31.961127
633.883116	33490.021263	31.966144
634.454129	33521.461662	31.971162
634.715473	33565.883030	31.976180
635.537529	33609.234798	31.981197
636.334544	33664.712143	31.986215
636.871759	33711.716032	31.991232
637.449895	33758.209132	31.996250
637.824930	33807.461665	32.001268
638.854241	33841.796255	32.006285
639.432021	33902.369174	32.011303
639.872247	33957.385716	32.016320
640.608684	33994.013477	32.021338
641.351839	34056.132193	32.026356
641.989452	34093.704353	32.031373
642.396847	34151.748547	32.036391
643.263840	34200.878202	32.041408
644.051501	34242.320309	32.046426
644.504044	34306.986285	32.051444
645.553266	34339.520154	32.056461
646.037721	34407.496462	32.061479
646.461234	34450.978530	32.066496
647.024953	34500.937654	32.071514
648.077528	34550.560566	32.076532
648.368457	34599.396925	32.081549
649.115121	34659.959909	32.086567
650.147966	34692.771369	32.091584
650.780764	34731.557968	32.096602
651.393201	34806.120506	32.101620
652.107886	34836.454409	32.106637
652.521426	34897.539487	32.111655
652.976402	34949.960671	32.116672
653.544468	34994.608165	32.121690
654.257545	35060.603898	32.126708
655.397079	35100.324296	32.131725
655.758653	35166.370113	32.136743
656.503201	35205.609795	32.141760
657.304040	35264.110716	32.146778
657.771133	35306.809334	32.151796
658.465010	35371.185644	32.156813
659.405272	35411.558053	32.161831
659.829995	35475.417990	32.166848
660.371870	35509.370186	32.171866
660.968671	35570.800594	32.176884
661.739254	35625.989186	32.181901
662.170785	35684.466836	32.186919
663.028352	35728.409668	32.191936
663.638670	35793.980109	32.196954
663.862582	35859.547696	32.201972
664.590952	35901.235129	32.206989
665.360190	35970.797824	32.212007
666.351879	36019.429026	32.217024
666.965721	36074.765451	32.222042
667.581167	36137.516077	32.227060
668.216367	36172.801097	32.232077
668.957537	36244.335299	32.237095
669.685218	36285.881918	32.242112
670.500495	36343.548777	32.247130
671.073373	36384.719854	32.252148
671.862247	36433.203256	32.257165
672.158112	36486.953662	32.262183
672.735059	36529.352566	32.267200
673.366357	36575.509278	32.272218
673.931884	36635.220691	32.277236
674.464555	36679.523610	32.282253
675.013664	36750.586061	32.287271
675.462629	36807.325919	32.292288
676.431874	36869.174767	32.297306
677.196578	36929.730513	32.302324
677.992865	36986.723109	32.307341
678.456977	37042.671485	32.312359
679.022833	37104.380473	32.317376
679.890168	37159.535077	32.322394
680.352345	37225.807920	32.327412
681.955182	37273.711676	32.332429
682.412337	37341.453596	32.337447
683.003698	37413.754498	32.342464
684.135491	37445.920264	32.347482
684.670758	37509.730943	32.352500
685.212314	37561.555295	32.357517
685.695001	37616.466777	32.362535
686.530694	37664.276217	32.367552
687.194631	37731.211076	32.372570
687.800149	37787.019591	32.377588
688.648095	37833.507903	32.382605
689.682317	37893.023035	32.387623
689.781749	37951.674987	32.392640
690.761674	37990.133242	32.397658
691.381156	38059.257021	32.402676
692.270579	38108.142349	32.407693
692.919492	38167.133271	32.412711
693.393691	38228.801064	32.417728
694.037983	38283.729986	32.422746
694.811758	38334.400288	32.427764
695.703841	38398.977414	32.432781
696.288807	38458.922411	32.437799
696.501213	38522.343693	32.442816
697.593893	38565.974309	32.447834
698.063665	38633.148637	32.452852
698.694221	38691.702830	32.457869
699.540898	38758.683627	32.462887
700.549744	38811.265216	32.467904
701.190879	38869.804152	32.472922
701.803686	38936.821313	32.477940
702.884775	38974.707540	32.482957
703.470265	39046.215380	32.487975
704.069771	39100.182797	32.492992
704.947044	39141.778892	32.498010
705.761646	39211.899655	32.503028
706.188304	39260.781585	32.508045
706.475252	39320.796005	32.513063
707.137666	39375.441768	32.518080
707.828300	39423.015967	32.523098
708.516446	39490.362337	32.528116
709.345862	39540.535434	32.533133
710.288112	39587.093986	32.538151
710.313482	39649.716703	32.543168
711.043984	39684.900893	32.548186
711.945746	39752.219025	32.553204
712.619970	39813.625799	32.558221
713.351786	39860.373134	32.563239
713.970706	39936.679329	32.568256
714.695816	39991.140488	32.573274
715.411668	40058.402705	32.578292
716.090029	40116.031744	32.583309
716.982874	40194.457376	32.588327
717.305879	40247.870098	32.593344
718.368754	40303.713449	32.598362
719.063332	40367.558429	32.603380
719.906409	40438.979090	32.608397
720.556491	40503.807766	32.613415
721.482670	40577.306756	32.618432
722.254968	40628.018850	32.623450
722.720572	40694.274770	32.628468
723.782039	40756.014375	32.633485
724.678095	40816.124755	32.638503
725.174749	40882.113113	32.643520
725.962054	40937.193444	32.648538
726.424768	41002.929053	32.653556
727.281322	41062.622391	32.658573
728.188912	41132.368843	32.663591
728.807978	41196.266796	32.668608
729.620915	41247.004226	32.673626
730.059728	41319.440694	32.678644
731.039600	41378.150391	32.683661
731.719262	41446.247034	32.688679
732.569521	41514.304174	32.693696
733.402381	41570.580972	32.698714
734.403994	41635.772739	32.703732
735.043643	41689.453386	32.708749
735.389186	41753.097330	32.713767
736.239100	41810.640128	32.718784
737.373428	41872.922559	32.723802
738.057757	41938.926121	32.728820
738.766203	41996.700234	32.733837
739.601826	42052.546068	32.738855
740.234457	42118.132746	32.743872
741.073525	42158.930126	32.748890
741.686931	42224.119698	32.753908
741.736272	42284.907814	32.758925
742.612409	42345.861016	32.763943
743.261672	42423.195432	32.768960
744.514347	42487.183432	32.773978
744.737535	42563.952319	32.778996
745.312825	42624.153236	32.784013
746.290069	42689.491677	32.789031
746.819259	42759.245062	32.794048
747.707571	42806.729417	32.799066
748.646876	42879.118029	32.804084
749.313633	42945.995677	32.809101
749.811011	43006.122015	32.814119
750.789767	43065.531613	32.819136
751.669382	43115.159963	32.824154
752.194389	43186.363565	32.829172
752.869900	43247.392908	32.834189
753.694200	43315.619040	32.839207
754.384581	43382.440998	32.844224
754.980105	43450.212004	32.849242
755.548030	43514.262362	32.854260
756.443799	43573.929811	32.859277
757.236467	43650.732747	32.864295
757.723858	43722.348309	32.869312
758.640746	43796.816788	32.874330
759.379082	43874.723950	32.879348
760.288407	43949.591749	32.884365
761.297981	44011.671519	32.889383
761.718320	44090.125520	32.894400
763.001059	44160.546925	32.899418
763.629521	44217.868052	32.904436
764.386620	44292.010797	32.909453
765.199126	44360.993708	32.914471
765.892980	44442.348932	32.919488
766.690514	44494.640972	32.924506
767.346317	44577.037576	32.929524
767.943560	44647.226233	32.934541
769.139449	44732.392490	32.939559
769.983260	44790.920986	32.944576
770.428952	44864.248233	32.949594
771.437807	44920.157803	32.954612
772.063056	45000.879869	32.959629
773.286461	45067.806456	32.964647
773.802590	45137.836502	32.969664
774.791570	45202.974377	32.974682
775.415631	45285.521354	32.979700
776.186561	45351.132995	32.984717
777.192930	45398.570984	32.989735
777.863364	45482.278754	32.994752
778.772542	45546.499977	32.999770
779.384548	45615.336811	33.004788
780.179441	45680.381179	33.009805
780.970564	45751.145990	33.014823
781.366663	45824.579817	33.019840
782.510397	45892.941917	33.024858
783.379628	45973.421438	33.029876
783.740392	46036.387810	33.034893
784.925806	46100.724848	33.039911
785.631729	46176.281364	33.044928
786.285231	46236.469763	33.049946
787.065016	46308.469034	33.054964
787.889020	46375.035162	33.059981
789.156185	46444.843646	33.064999
789.683097	46502.336745	33.070016
790.702584	46558.382395	33.075034
791.506456	46617.320910	33.080052
791.833473	46693.290168	33.085069
792.653259	46728.129100	33.090087
793.275088	46801.890766	33.095104
793.979226	46848.213475	33.100122
794.836908	46926.616944	33.105140
795.649076	46985.340839	33.110157
796.087080	47060.615699	33.115175
797.050203	47134.422245	33.120192
797.889295	47197.931888	33.125210
798.473309	47268.697946	33.130228
799.158201	47350.383663	33.135245
800.366518	47406.102243	33.140263
801.041624	47489.086897	33.145280
801.962097	47553.695464	33.150298
802.529983	47640.310481	33.155316
803.163349	47706.520777	33.160333
804.297617	47778.450734	33.165351
804.770320	47873.850174	33.170368
805.582038	47941.976543	33.175386
806.795894	48017.718872	33.180404
807.048115	48092.567061	33.185421
808.281748	48185.158850	33.190439
809.021866	48250.981887	33.195456
809.686897	48334.530602	33.200474
810.542944	48414.351357	33.205492
811.214049	48494.867669	33.210509
812.208291	48572.193416	33.215527
813.221171	48652.078632	33.220544
814.122900	48714.441564	33.225562
815.146140	48782.348197	33.230580
815.957440	48873.379520	33.235597
817.190494	48934.967928	33.240615
817.832823	49017.270813	33.245632
818.547506	49081.081566	33.250650
819.324925	49149.593546	33.255668
820.001607	49230.355284	33.260685
821.334120	49294.014831	33.265703
821.432830	49377.374620	33.270720
822.371642	49440.292722	33.275738
823.070197	49522.421767	33.280756
824.049230	49605.699316	33.285773
824.882125	49683.806603	33.290791
826.055501	49763.289480	33.295808
826.820102	49831.591564	33.300826
827.496257	49904.597080	33.305844
828.254673	49971.199862	33.310861
829.141328	50036.864223	33.315879
829.877654	50130.794940	33.320896
830.710356	50195.707986	33.325914
832.069431	50261.171767	33.330932
832.312827	50355.639680	33.335949
833.320265	50418.162189	33.340967
834.214822	50482.993861	33.345984
834.812215	50541.151577	33.351002
835.659985	50607.919239	33.356020
836.622563	50667.016428	33.361037
837.542878	50735.966200	33.366055
838.172924	50797.634964	33.371072
839.102010	50870.556853	33.376090
840.192650	50925.339632	33.381108
840.583074	51000.294844	33.386125
841.487906	51076.736894	33.391143
842.432287	51153.621093	33.396160
843.516904	51205.256269	33.401178
844.252745	51276.654791	33.406196
844.506564	51352.911301	33.411213
845.562357	51412.526297	33.416231
846.401953	51495.487743	33.421248
846.989609	51572.184361	33.426266
848.123547	51641.532824	33.431284
848.785832	51728.345267	33.436301
850.102885	51798.652974	33.441319
850.812939	51894.402295	33.446336
851.236691	51957.101986	33.451354
851.943761	52032.746444	33.456372
852.940122	52117.222738	33.461389
854.295070	52206.552974	33.466407
854.870455	52283.425006	33.471424
855.618351	52371.154778	33.476442
856.846782	52435.419668	33.481460
857.687471	52526.698511	33.486477
858.626279	52602.362140	33.491495
859.285845	52673.674217	33.496512
860.119472	52752.274517	33.501530
861.093014	52838.165416	33.506548
861.722887	52918.761921	33.511565
863.014655	53002.952352	33.516583
863.943306	53076.820639	33.521600
864.698437	53152.443222	33.526618
865.731758	53229.123330	33.531636
866.361608	53303.633445	33.536653
867.309322	53376.991795	33.541671
868.284994	53468.367548	33.546688
869.207106	53543.580148	33.551706
869.791631	53621.497965	33.556724
870.319318	53719.012432	33.561741
871.726538	53786.106887	33.566759
872.265789	53880.896589	33.571776
872.854842	53960.601561	33.576794
874.112436	54030.220467	33.581812
875.009884	54130.550484	33.586829
876.141036	54208.210244	33.591847
876.987540	54274.868649	33.596864
877.995034	54361.269551	33.601882
878.808700	54435.811889	33.606900
879.665791	54525.883047	33.611917
880.783843	54596.350138	33.616935
881.447319	54649.602526	33.621952
882.074010	54730.258108	33.626970
883.113641	54791.439803	33.631988
883.928743	54857.698176	33.637005
884.270953	54940.631523	33.642023
885.550404	55011.809985	33.647040
886.373415	55085.823229	33.652058
886.830228	55162.697961	33.657076
887.592689	55255.770626	33.662093
888.360152	55330.185102	33.667111
889.370605	55417.174501	33.672128
889.957681	55507.397650	33.677146
891.187648	55585.871425	33.682164
891.627975	55685.288464	33.687181
892.532981	55765.743360	33.692199
893.778832	55863.316029	33.697216
894.923367	55949.301784	33.702234
896.082710	56020.260248	33.707252
896.788810	56111.332344	33.712269
898.009040	56183.714851	33.717287
899.102152	56276.203479	33.722304
899.622345	56360.633291	33.727322
900.946514	56424.679308	33.732340
901.863036	56513.668100	33.737357
902.730387	56594.606138	33.742375
903.781597	56669.315528	33.747392
904.705090	56742.845996	33.752410
905.745830	56822.352716	33.757428
906.259579	56900.570457	33.762445
907.374134	56980.400730	33.767463
908.337857	57057.098590	33.772480
909.125978	57139.847839	33.777498
910.197953	57227.543179	33.782516
910.836098	57305.862809	33.787533
911.651167	57383.545355	33.792551
912.619376	57469.518954	33.797568
913.376590	57553.540872	33.802586
914.437367	57650.865239	33.807604
914.956971	57737.523903	33.812621
915.957717	57828.466085	33.817639
916.985535	57912.910647	33.822656
917.657335	58014.238648	33.827674
918.766849	58104.328298	33.832692
919.687925	58187.856649	33.837709
920.803723	58274.615545	33.842727
921.708060	58368.739014	33.847744
922.731218	58451.690373	33.852762
923.619024	58541.302842	33.857780
924.209356	58630.552664	33.862797
925.382451	58718.068526	33.867815
926.482693	58805.059695	33.872832
927.030403	58908.376029	33.877850
927.792076	58987.014629	33.882868
928.821378	59077.989987	33.887885
930.031994	59170.351333	33.892903
930.619364	59267.835312	33.897920
931.310296	59345.226988	33.902938
932.557504	59411.764548	33.907956
933.313127	59487.296425	33.912973
934.114400	59588.577707	33.917991
935.560994	59653.812063	33.923008
935.965206	59749.051364	33.928026
937.033611	59832.655250	33.933044
937.926325	59924.853082	33.938061
938.718019	60004.949864	33.943079
939.986696	60088.993469	33.948096
940.542432	60182.714328	33.953114
941.781853	60271.669847	33.958132
942.610918	60373.456145	33.963149
943.628789	60477.012643	33.968167
944.695332	60556.142961	33.973184
945.402170	60653.318390	33.978202
946.660196	60738.812698	33.983220
947.700439	60833.795311	33.988237
948.633019	60911.938083	33.993255
949.659742	61002.159161	33.998272
950.428629	61108.300505	34.003290
951.633630	61181.140748	34.008308
952.388019	61283.995319	34.013325
953.353669	61368.178150	34.018343
954.562849	61461.236258	34.023360
955.033069	61558.270894	34.028378
956.282517	61653.214906	34.033396
957.338952	61746.595542	34.038413
958.205169	61832.940260	34.043431
959.082382	61925.440919	34.048448
959.501223	62023.916519	34.053466
960.847256	62121.762001	34.058484
961.677791	62224.606449	34.063501
962.556804	62316.884553	34.068519
963.843036	62422.786816	34.073536
964.743234	62516.893978	34.078554
965.632691	62619.273341	34.083572
966.890500	62722.055682	34.088589
967.750810	62821.153591	34.093607
968.721496	62921.317569	34.098624
969.204804	63014.025181	34.103642
970.434566	63121.140301	34.108660
971.525151	63217.832156	34.113677
972.422970	63326.112795	34.118695
973.723465	63424.742793	34.123712
974.783830	63530.895624	34.128730
975.722763	63618.225354	34.133748
976.407051	63728.272774	34.138765
977.513651	63818.662009	34.143783
978.613051	63910.110723	34.148800
979.047772	64030.260726	34.153818
980.601609	64115.056989	34.158836
981.846037	64218.004325	34.163853
982.756681	64306.355431	34.168871
983.909148	64390.837824	34.173888
984.655548	64478.985328	34.178906
985.611647	64553.368784	34.183924
986.774319	64637.844336	34.188941
987.553467	64712.777643	34.193959
988.695299	64788.165153	34.198976
989.511945	64877.822356	34.203994
990.614581	64962.065726	34.209012
991.780254	65051.314513	34.214029
992.193238	65124.940232	34.219047
993.313942	65218.839392	34.224064
994.069104	65317.231210	34.229082
995.086601	65395.502186	34.234100
995.931565	65504.596333	34.239117
997.080035	65602.721768	34.244135
998.155804	65693.863831	34.249152
998.675652	65802.922968	34.254170
999.505661	65894.635665	34.259188
1001.024909	65994.614864	34.264205
1001.518422	66109.680632	34.269223
1002.978589	66206.104635	34.274240
1003.815171	66310.100893	34.279258
1004.933942	66406.475988	34.284276
1005.744928	66515.360207	34.289293
1006.724516	66613.602958	34.294311
1007.982068	66724.820837	34.299328
1008.807349	66834.895300	34.304346
1009.892563	66945.800765	34.309364
1011.112477	67043.795868	34.314381
1012.235250	67158.259295	34.319399
1013.376724	67254.887706	34.324416
1014.298980	67371.023539	34.329434
1015.284417	67468.527475	34.334452
1016.394996	67570.073852	34.339469
1017.327862	67676.336302	34.344487
1018.463587	67772.497596	34.349504
1019.210001	67884.387805	34.354522
1020.602187	67973.124563	34.359540
1021.749002	68082.747533	34.364557
1022.580730	68188.750928	34.369575
1023.661876	68282.573426	34.374592
1024.745189	68387.312335	34.379610
1025.694831	68486.141092	34.384628
1026.882304	68591.591029	34.389645
1027.831505	68690.496705	34.394663
1029.060351	68801.753215	34.399680
1029.551841	68896.019935	34.404698
1030.877611	69007.236934	34.409716
1032.329512	69101.295018	34.414733
1033.247002	69217.474256	34.419751
1034.184532	69303.301211	34.424768
1035.314107	69392.983339	34.429786
1036.207992	69501.789034	34.434804
1037.230147	69600.675094	34.439821
1038.677126	69698.603281	34.444839
1039.631701	69784.574951	34.449856
1040.723592	69861.730801	34.454874
1041.728145	69948.484967	34.459892
1042.919583	70035.828939	34.464909
1043.953686	70113.614125	34.469927
1044.837204	70202.448295	34.474944
1045.557888	70296.830633	34.479962
1046.482133	70373.939357	34.484980
1047.678290	70476.409721	34.489997
1048.240490	70558.656419	34.495015
1049.341350	70659.348583	34.500032
1050.343238	70758.268993	34.505050
1051.341187	70855.149780	34.510068
1052.336864	70956.719463	34.515085
1053.353186	71060.333474	34.520103
1054.496376	71155.562554	34.525120
1055.542544	71270.735234	34.530138
1056.604093	71367.551567	34.535156
1057.669297	71470.566047	34.540173
1058.199063	71596.475428	34.545191
1059.501091	71691.700792	34.550208
1060.712202	71804.405147	34.555226
1061.746077	71921.011543	34.560244
1062.836254	72031.291191	34.565261
1063.747712	72139.078795	34.570279
1064.813587	72252.276377	34.575296
1065.871282	72370.480229	34.580314
1067.199760	72476.958582	34.585332
1068.598986	72589.782824	34.590349
1069.289949	72713.992915	34.595367
1070.911868	72807.169750	34.600384
1072.021022	72914.734251	34.605402
1072.960217	73026.256659	34.610420
1074.254352	73128.744181	34.615437
1075.547054	73237.740888	34.620455
1076.210728	73338.579444	34.625472
1077.437764	73450.235379	34.630490
1078.308471	73555.768667	34.635508
1079.396890	73657.217410	34.640525
1080.429346	73770.049825	34.645543
1081.776223	73882.826551	34.650560
1082.964392	73985.588105	34.655578
1083.745952	74096.680287	34.660596
1085.132457	74206.236100	34.665613
1085.967788	74310.540451	34.670631
1086.963272	74415.306455	34.675648
1088.149032	74521.793183	34.680666
1089.259855	74638.175789	34.685684
1090.332695	74747.335785	34.690701
1091.229419	74864.189790	34.695719
1092.526736	74967.703679	34.700736
1093.968194	75081.154622	34.705754
1094.570915	75184.413574	34.710772
1096.217252	75294.780834	34.715789
1096.911493	75404.402750	34.720807
1098.116301	75498.220949	34.725824
1098.958644	75596.975970	34.730842
1100.187970	75690.702695	34.735860
1101.246441	75793.393039	34.740877
1101.635548	75902.560623	34.745895
1103.136135	75993.850451	34.750912
1104.308752	76106.913881	34.755930
1104.971327	76210.282330	34.760948
1106.386219	76317.923943	34.765965
1107.600420	76424.188719	34.770983
1108.767067	76529.083879	34.776000
1109.695476	76630.851187	34.781018
1110.255096	76743.996714	34.786036
1111.567850	76863.924538	34.791053
1112.650692	76993.407621	34.796071
1113.819404	77094.014072	34.801088
1115.112956	77212.853644	34.806106
1115.886349	77337.262526	34.811124
1117.403220	77446.726772	34.816141
1118.321688	77567.979183	34.821159
1119.565764	77690.261299	34.826176
1120.824302	77803.611272	34.831194
1121.830301	77924.978297	34.836212
1123.243133	78036.036028	34.841229
1124.366250	78150.332242	34.846247
1125.650479	78275.443029	34.851264
1126.694031	78377.624248	34.856282
1127.887900	78495.867764	34.861300
1129.324882	78600.686390	34.866317
1130.585001	78723.522044	34.871335
1131.745596	78835.452239	34.876352
1132.986889	78946.112404	34.881370
1133.897802	79050.599837	34.886388
1135.226612	79151.525992	34.891405
1136.333583	79268.232899	34.896423
1137.427924	79379.399153	34.901440
1138.575989	79484.489483	34.906458
1139.708296	79594.336135	34.911476
1141.046167	79697.678103	34.916493
1142.121013	79819.310897	34.921511
1143.194361	79922.240955	34.926528
1144.651785	80030.925754	34.931546
1145.604142	80138.806502	34.936564
1146.977699	80235.091247	34.941581
1147.911842	80355.163002	34.946599
1149.182633	80456.566238	34.951616
1150.636136	80571.916970	34.956634
1151.528515	80684.317089	34.961652
1152.692789	80784.803343	34.966669
1153.627237	80897.690987	34.971687
1154.690282	80996.013536	34.976704
1155.940389	81114.661422	34.981722
1156.786428	81228.190738	34.986740
1157.907510	81346.658188	34.991757
1158.712879	81453.918075	34.996775
1159.964363	81561.284576	35.001792
1161.397731	81663.502312	35.006810
1162.130624	81778.740468	35.011828
1163.422863	81877.504867	35.016845
1164.421365	81982.992029	35.021863
1165.647521	82090.542300	35.026880
1166.924560	82213.010438	35.031898
1167.359666	82316.433197	35.036916
1168.644449	82425.960885	35.041933
1169.463261	82551.860708	35.046951
1170.857322	82668.730812	35.051968
1172.178460	82790.531544	35.056986
1173.206119	82916.166446	35.062004
1174.415517	83027.631126	35.067021
1175.976614	83142.188797	35.072039
1177.257225	83260.028541	35.077056
1178.481934	83387.872918	35.082074
1179.819425	83504.781983	35.087092
1180.944413	83628.155038	35.092109
1182.216066	83741.737839	35.097127
1183.281252	83868.687486	35.102144
1185.059581	83975.375715	35.107162
1186.036591	84100.728630	35.112180
1187.280888	84206.440816	35.117197
1188.451079	84331.208029	35.122215
1189.628397	84435.933098	35.127232
1190.523112	84552.646539	35.132250
1191.595512	84690.392252	35.137268
1193.082606	84806.247897	35.142285
1194.157767	84916.378304	35.147303
1195.299262	85059.407336	35.152320
1196.434765	85168.302896	35.157338
1197.913467	85300.051121	35.162356
1198.905539	85421.887814	35.167373
1199.724822	85559.129364	35.172391
1201.310720	85677.357714	35.177408
1202.717536	85800.154913	35.182426
1203.940675	85930.771668	35.187444
1205.147960	86042.195734	35.192461
1206.351028	86162.498307	35.197479
1207.477477	86306.884909	35.202496
1208.778946	86417.094619	35.207514
1209.817457	86545.291217	35.212532
1211.181542	86664.426573	35.217549
1212.289300	86801.997008	35.222567
1213.487577	86911.138121	35.227584
1214.951885	87052.655974	35.232602
1216.019211	87171.246973	35.237620
1217.429712	87293.660167	35.242637
1218.878539	87432.147875	35.247655
1219.955101	87542.974571	35.252672
1221.085827	87665.017038	35.257690
1222.462916	87788.728324	35.262708
1223.677215	87907.717373	35.267725
1224.865175	88032.041880	35.272743
1226.133670	88139.369606	35.277760
1227.294181	88240.461150	35.282778
1228.254132	88357.596097	35.287796
1229.434697	88457.983569	35.292813
1231.016865	88564.530022	35.297831
1231.863143	88691.480021	35.302848
1233.193582	88792.781117	35.307866
1234.401363	88904.510895	35.312884
1235.496975	89023.746314	35.317901
1236.857535	89140.625791	35.322919
1237.910767	89251.212049	35.327936
1239.067189	89371.641230	35.332954
1239.905408	89509.037867	35.337972
1241.284786	89629.603780	35.342989
1242.676245	89746.095861	35.348007
1243.892084	89866.764981	35.353024
1244.892194	90006.655952	35.358042
1245.954836	90140.776719	35.363060
1247.228251	90271.253780	35.368077
1248.582278	90406.879253	35.373095
1249.941043	90538.438413	35.378112
1251.545202	90678.168106	35.383130
1252.436068	90800.803967	35.388148
1253.818970	90943.429070	35.393165
1255.280951	91071.294335	35.398183
1256.159660	91215.481249	35.403200
1257.717609	91341.941494	35.408218
1258.781882	91486.739453	35.413236
1260.230111	91615.141335	35.418253
1261.815857	91757.024838	35.423271
1263.123703	91896.139034	35.428288
1264.486729	92020.869653	35.433306
1265.433886	92162.167920	35.438324
1266.454062	92292.324155	35.443341
1268.307234	92428.920055	35.448359
1269.297862	92555.686203	35.453376
1270.833400	92693.491661	35.458394
1271.975285	92827.774414	35.463412
1273.249424	92956.951812	35.468429
1274.443785	93095.180856	35.473447
1276.011317	93227.247926	35.478464
1277.731530	93356.647695	35.483482
1278.931631	93494.897302	35.488500
1280.451850	93615.930833	35.493517
1281.903173	93735.091119	35.498535
1282.492924	93876.786075	35.503552
1283.945487	93989.160728	35.508570
1285.238505	94123.294491	35.513588
1286.551361	94249.639615	35.518605
1287.897152	94381.723517	35.523623
1289.042720	94514.997552	35.528640
1290.525988	94638.439806	35.533658
1291.496745	94780.143200	35.538676
1292.668533	94898.462290	35.543693
1293.970043	95034.086651	35.548711
1295.307689	95148.971313	35.553728
1296.569934	95256.986448	35.558746
1297.735341	95384.430447	35.563764
1299.163285	95502.857506	35.568781
1300.361245	95621.188914	35.573799
1301.621679	95742.534653	35.578816
1302.897236	95860.146522	35.583834
1304.314966	95987.958687	35.588852
1305.202977	96098.833316	35.593869
1306.779877	96233.371101	35.598887
1307.851864	96358.494963	35.603904
1308.918997	96494.696785	35.608922
1310.130701	96625.727209	35.613940
1311.661948	96757.213674	35.618957
1312.824555	96887.266585	35.623975
1314.043322	97041.033672	35.628992
1315.446184	97176.117156	35.634010
1316.594245	97315.284288	35.639028
1317.906045	97462.903197	35.644045
1319.301663	97596.668193	35.649063
1320.696158	97750.703172	35.654080
1322.171776	97886.317053	35.659098
1323.624774	98041.394857	35.664116
1324.679670	98184.605624	35.669133
1326.333661	98323.881990	35.674151
1327.388376	98467.404555	35.679168
1328.902027	98604.243990	35.684186
1330.007036	98756.908360	35.689204
1331.599176	98889.858926	35.694221
1333.183338	99035.546813	35.699239
1334.353141	99179.738831	35.704256
1335.807200	99315.503836	35.709274
1337.200266	99467.665327	35.714292
1338.719319	99615.050142	35.719309
1340.227270	99752.700851	35.724327
1341.280390	99890.171608	35.729344
1342.753074	100037.408338	35.734362
1344.057674	100191.423461	35.739380
1345.053880	100321.819789	35.744397
1347.180037	100455.270312	35.749415
1348.341473	100616.675558	35.754432
1349.806096	100752.143686	35.759450
1351.363266	100900.751795	35.764468
1352.310905	101027.540771	35.769485
1353.791303	101176.276741	35.774503
1355.191477	101315.510392	35.779520
1356.640043	101449.460319	35.784538
1358.019810	101603.586807	35.789556
1359.505557	101733.812063	35.794573
1361.131332	101875.740273	35.799591
1362.624477	102000.378847	35.804608
1363.732187	102137.677136	35.809626
1364.936628	102273.125913	35.814644
1366.206647	102406.932575	35.819661
1367.748787	102537.817756	35.824679
1368.735427	102661.983556	35.829696
1370.089892	102787.869599	35.834714
1371.260645	102901.484708	35.839732
1372.726337	103039.459084	35.844749
1374.227865	103157.793891	35.849767
1374.979002	103298.737126	35.854784
1376.279274	103421.496664	35.859802
1377.665032	103571.832257	35.864820
1378.946759	103703.562651	35.869837
1380.527487	103842.396710	35.874855
1381.735129	103986.853077	35.879872
1383.290887	104125.230842	35.884890
1384.740413	104278.022375	35.889908
1385.990408	104407.230576	35.894925
1387.286094	104551.341031	35.899943
1388.927614	104709.553274	35.904960
1389.833088	104839.451400	35.909978
1391.575575	104998.737966	35.914996
1392.993166	105139.453410	35.920013
1394.367899	105282.043325	35.925031
1395.438633	105441.173838	35.930048
1397.191045	105589.255461	35.935066
1398.665917	105745.336833	35.940084
1399.799085	105890.955771	35.945101
1401.562196	106047.043945	35.950119
1402.562956	106196.628398	35.955136
1403.886406	106366.363077	35.960154
1405.345201	106517.237379	35.965172
1406.936978	106675.103572	35.970189
1408.291889	106832.502159	35.975207
1409.723309	106987.820149	35.980224
1411.299703	107141.863025	35.985242
1412.714718	107310.336769	35.990260
1414.446659	107460.116710	35.995277
1415.936093	107608.062789	36.000295
1417.366528	107770.575556	36.005312
1418.841320	107921.582737	36.010330
1420.444554	108060.501148	36.015348
1421.914136	108218.839944	36.020365
1423.712378	108359.918925	36.025383
1425.138381	108510.108445	36.030400
1426.349805	108660.649451	36.035418
1427.820939	108804.371612	36.040436
1429.206699	108961.165295	36.045453
1431.077301	109091.755926	36.050471
1432.019870	109250.077623	36.055488
1433.533834	109392.733153	36.060506
1434.946985	109530.399039	36.065524
1436.582181	109694.215027	36.070541
1438.047340	109821.190315	36.075559
1439.526566	109972.045018	36.080576
1440.434172	110120.333102	36.085594
1441.976868	110277.774933	36.090612
1443.883315	110415.601630	36.095629
1445.463953	110562.025833	36.100647
1446.805081	110688.987369	36.105664
1447.972100	110819.274984	36.110682
1449.035301	110941.053686	36.115700
1450.408613	111095.419814	36.120717
1451.880775	111215.128368	36.125735
1453.112587	111366.125927	36.130752
1454.424507	111519.523354	36.135770
1455.925882	111651.971375	36.140788
1457.081289	111799.369371	36.145805
1458.311646	111948.319836	36.150823
1459.829913	112099.181422	36.155840
1461.549441	112250.208181	36.160858
1462.930592	112409.620004	36.165876
1464.297743	112572.940758	36.170893
1466.058111	112717.260290	36.175911
1467.400395	112880.561701	36.180928
1468.713924	113039.184382	36.185946
1470.577024	113193.181949	36.190964
1471.760912	113355.194950	36.195981
1473.292398	113507.322736	36.200999
1474.557401	113665.919140	36.206016
1476.483818	113814.472685	36.211034
1478.252514	113984.810001	36.216052
1479.861938	114142.753315	36.221069
1481.637551	114302.063944	36.226087
1483.006902	114454.944948	36.231104
1484.399971	114623.902921	36.236122
1486.182711	114752.707977	36.241140
1487.247364	114917.358275	36.246157
1488.725076	115059.033053	36.251175
1490.135836	115226.662811	36.256192
1491.754026	115378.990777	36.261210
1493.543225	115538.402052	36.266228
1494.338096	115705.246522	36.271245
1496.374757	115864.259677	36.276263
1497.876621	116025.834216	36.281280
1499.534419	116179.585190	36.286298
1500.874740	116330.950078	36.291316
1502.217264	116490.761206	36.296333
1503.945268	116657.697942	36.301351
1505.569041	116821.651354	36.306368
1506.958097	116977.893696	36.311386
1508.845602	117132.310378	36.316404
1509.946400	117290.791051	36.321421
1511.953928	117437.998163	36.326439
1513.182929	117609.661284	36.331456
1514.661401	117763.038776	36.336474
1516.240824	117918.876748	36.341492
1517.781143	118078.894334	36.346509
1519.487220	118232.953938	36.351527
1521.142023	118389.207006	36.356544
1522.553122	118548.849161	36.361562
1524.035524	118706.967716	36.366580
1525.334923	118874.930431	36.371597
1526.856438	119017.797974	36.376615
1528.274620	119164.950332	36.381632
1529.480397	119312.618488	36.386650
1531.478920	119442.989624	36.391668
1532.770319	119587.283546	36.396685
1534.291339	119727.324749	36.401703
1535.455419	119881.296679	36.406720
1536.812507	120030.768489	36.411738
1538.446264	120170.965140	36.416756
1539.836098	120331.552482	36.421773
1541.430798	120490.119996	36.426791
1542.713314	120650.511062	36.431808
1544.194508	120815.785309	36.436826
1545.811984	120981.418885	36.441844
1547.375404	121140.438574	36.446861
1549.218440	121314.245012	36.451879
1550.452368	121482.120992	36.456896
1552.005124	121648.718919	36.461914
1554.049345	121802.663683	36.466932
1555.348383	121979.714482	36.471949
1556.910216	122140.703544	36.476967
1558.786108	122309.534021	36.481984
1559.943872	122483.963656	36.487002
1561.879804	122649.835800	36.492020
1563.391280	122816.029717	36.497037
1564.862903	122976.987548	36.502055
1566.408226	123156.983477	36.507072
1568.082523	123324.294610	36.512090
1569.895055	123500.818068	36.517108
1571.215027	123668.706944	36.522125
1572.825007	123839.425942	36.527143
1574.540014	124005.265664	36.532160
1576.207835	124185.033773	36.537178
1578.031570	124344.145386	36.542196
1579.767179	124517.280641	36.547213
1581.257019	124676.333274	36.552231
1582.888612	124859.721533	36.557248
1584.400260	125029.146460	36.562266
1586.235162	125186.386687	36.567284
1587.439957	125368.009580	36.572301
1588.946841	125528.014538	36.577319
1590.813555	125700.338605	36.582336
1592.385843	125877.764566	36.587354
1593.836452	126038.262825	36.592372
1595.532539	126225.158844	36.597389
1597.115970	126387.652115	36.602407
1598.699081	126574.201145	36.607424
1600.356471	126736.203410	36.612442
1602.394510	126907.532585	36.617460
1603.569136	127081.837454	36.622477
1604.960674	127254.601567	36.627495
1606.920455	127428.150573	36.632512
1608.506296	127598.985887	36.637530
1609.964061	127771.236049	36.642548
1611.602796	127946.245445	36.647565
1613.293156	128106.261786	36.652583
1614.777096	128266.197836	36.657600
1616.309560	128426.988529	36.662618
1617.829959	128572.631168	36.667636
1619.070257	128738.739970	36.672653
1620.822443	128893.215135	36.677671
1622.579368	129054.797275	36.682688
1624.027065	129217.772312	36.687706
1625.691052	129374.633150	36.692724
1626.957692	129556.096731	36.697741
1628.426056	129719.438826	36.702759
1630.413138	129889.363174	36.707776
1631.695214	130067.343786	36.712794
1633.851268	130221.128791	36.717812
1635.115198	130413.024772	36.722829
1636.718271	130583.711139	36.727847
1638.708419	130755.388601	36.732864
1639.958921	130937.345174	36.737882
1642.161506	131102.023046	36.742900
1643.629175	131295.818442	36.747917
1645.193080	131466.529089	36.752935
1646.984308	131642.969238	36.757952
1648.541565	131836.830155	36.762970
1650.281466	132007.452790	36.767988
1652.081526	132196.032430	36.773005
1653.617749	132376.622636	36.778023
1655.464162	132553.300448	36.783040
1657.102614	132724.703719	36.788058
1659.011944	132907.772035	36.793076
1660.656859	133088.666272	36.798093
1662.184629	133262.396316	36.803111
1664.333710	133436.218805	36.808128
1665.793480	133631.235141	36.813146
1667.844534	133798.727609	36.818164
1669.304396	133978.174458	36.823181
1670.861445	134164.106967	36.828199
1672.654280	134318.225431	36.833216
1674.034395	134517.555789	36.838234
1675.885318	134689.722721	36.843252
1677.623940	134890.759970	36.848269
1679.228583	135057.431067	36.853287
1681.258516	135242.383162	36.858304
1682.681581	135417.080563	36.863322
1684.737832	135585.799067	36.868340
1686.223795	135786.135085	36.873357
1687.780012	135954.440969	36.878375
1689.505443	136126.129556	36.883392
1691.425878	136311.726778	36.888410
1693.014589	136492.271240	36.893428
1694.809542	136666.600330	36.898445
1696.618486	136855.107850	36.903463
1698.078692	137024.018070	36.908480
1699.826629	137210.180625	36.913498
1701.661129	137377.436801	36.918516
1703.510184	137563.598221	36.923533
1704.929574	137739.298565	36.928551
1706.676467	137895.572262	36.933568
1708.085195	138053.383136	36.938586
1709.798994	138222.665506	36.943604
1711.345558	138385.588543	36.948621
1712.997988	138547.481878	36.953639
1714.857179	138718.543490	36.958656
1716.148442	138882.726369	36.963674
1717.710400	139056.549059	36.968692
1719.438939	139224.783003	36.973709
1721.123181	139410.564054	36.978727
1723.050438	139574.789176	36.983744
1724.291404	139753.926149	36.988762
1726.131978	139929.268474	36.993780
1728.244190	140116.595447	36.998797
1729.976483	140307.887252	37.003815
1731.771822	140476.244390	37.008832
1733.100411	140678.400257	37.013850
1735.255561	140854.179643	37.018868
1737.077089	141046.843394	37.023885
1738.797720	141224.987842	37.028903
1740.513714	141410.814293	37.033920
1742.041441	141598.522142	37.038938
1744.238291	141777.088512	37.043956
1745.789658	141980.523139	37.048973
1747.890928	142155.165347	37.053991
1749.769594	142332.860319	37.059008
1750.996599	142529.227333	37.064026
1752.953878	142715.644510	37.069044
1755.091343	142897.648932	37.074061
1756.860332	143086.012081	37.079079
1758.605461	143272.732508	37.084096
1760.385675	143464.011316	37.089114
1762.241360	143638.358809	37.094132
1763.876789	143836.963471	37.099149
1765.519069	144022.120463	37.104167
1767.814868	144199.633317	37.109184
1769.507587	144399.626741	37.114202
1771.545335	144572.493016	37.119220
1773.229018	144765.785208	37.124237
1774.754589	144938.151794	37.129255
1777.007683	145129.137713	37.134272
1778.434381	145317.391407	37.139290
1780.254686	145484.961024	37.144308
1781.687760	145677.880399	37.149325
1783.431685	145874.402148	37.154343
1785.738837	146048.856337	37.159360
1787.232286	146239.728837	37.164378
1789.345960	146425.788680	37.169396
1791.160612	146614.571686	37.174413
1792.660298	146799.197453	37.179431
1794.619053	146973.826188	37.184448
1796.095540	147176.913977	37.189466
1798.231268	147349.640656	37.194484
1800.192772	147548.153836	37.199501
1801.641739	147726.657835	37.204519
1803.767296	147887.017092	37.209536
1805.070187	148059.829161	37.214554
1806.835681	148218.586655	37.219572
1808.544721	148392.806521	37.224589
1810.519456	148557.249579	37.229607
1812.230440	148723.636848	37.234624
1813.915410	148902.173366	37.239642
1816.171613	149062.834731	37.244660
1818.042955	149232.710652	37.249677
1819.494502	149408.244617	37.254695
1821.265900	149583.183657	37.259712
1822.870884	149764.577313	37.264730
1824.713416	149938.543542	37.269748
1826.476468	150128.103549	37.274765
1828.085838	150310.399658	37.279783
1830.362314	150488.508807	37.284800
1831.687752	150682.819458	37.289818
1833.740338	150870.727830	37.294836
1835.809041	151059.091123	37.299853
1837.252662	151266.812002	37.304871
1839.713220	151445.531065	37.309888
1841.248471	151639.230950	37.314906
1843.084542	151833.949167	37.319924
1845.286396	152018.163896	37.324941
1847.169484	152214.347547	37.329959
1848.903199	152393.605544	37.334976
1850.514701	152603.526912	37.339994
1852.582951	152786.790946	37.345012
1854.418746	152987.766394	37.350029
1856.199091	153176.593339	37.355047
1858.436345	153375.795846	37.360064
1860.441714	153567.632122	37.365082
1862.171719	153764.584640	37.370100
1864.202994	153954.504577	37.375117
1866.434061	154147.157844	37.380135
1868.261876	154337.568693	37.385152
1870.005821	154527.841795	37.390170
1872.054563	154703.905247	37.395188
1874.486813	154890.533742	37.400205
1876.238709	155087.515945	37.405223
1878.032421	155260.288205	37.410240
1880.010508	155437.444447	37.415258
1881.714819	155620.972025	37.420276
1883.737014	155807.125485	37.425293
1885.754690	155995.207957	37.430311
1887.699861	156173.374957	37.435328
1889.523434	156357.027073	37.440346
1891.469807	156537.807781	37.445364
1893.599094	156715.289064	37.450381
1895.055227	156889.568702	37.455399
1897.381810	157056.914705	37.460416
1899.165948	157246.512021	37.465434
1901.096118	157422.266083	37.470452
1903.138834	157586.489751	37.475469
1904.883486	157766.497459	37.480487
1906.922465	157930.266883	37.485504
1908.797306	158099.997462	37.490522
1910.468908	158232.468560	37.495540
1912.378415	158396.945485	37.500557
1913.563351	158558.355422	37.505575
1915.307803	158715.911230	37.510592
1917.257320	158890.667963	37.515610
1918.804412	159057.957209	37.520628
1920.657705	159240.111041	37.525645
1922.364633	159424.863231	37.530663
1924.388299	159597.975945	37.535680
1926.211534	159798.473800	37.540698
1927.720959	159980.153475	37.545716
1929.462522	160167.846055	37.550733
1931.450295	160383.715799	37.555751
1933.741506	160577.714568	37.560768
1935.680169	160771.833761	37.565786
1937.145332	160979.141550	37.570804
1939.371979	161182.309735	37.575821
1941.015204	161391.925040	37.580839
1943.409076	161586.534444	37.585856
1945.521259	161809.887884	37.590874
1947.065697	162011.545845	37.595892
1949.473921	162205.699821	37.600909
1951.412102	162433.840403	37.605927
1953.562990	162631.055782	37.610944
1955.329451	162832.505589	37.615962
1957.529283	163045.732698	37.620980
1959.820424	163233.722031	37.625997
1961.601462	163449.250023	37.631015
1963.874957	163649.178177	37.636032
1966.600724	163850.329254	37.641050
1968.139777	164058.061649	37.646068
1970.357300	164239.232127	37.651085
1972.279493	164447.362512	37.656103
1974.319449	164628.068488	37.661120
1976.657036	164835.602506	37.666138
1978.932575	165019.798796	37.671156
1980.690510	165207.375650	37.676173
1982.537973	165416.525342	37.681191
1984.763779	165585.525714	37.686208
1986.536991	165788.601541	37.691226
1988.503178	165971.456569	37.696244
1990.998549	166152.186564	37.701261
1992.728435	166347.104462	37.706279
1994.685776	166540.401897	37.711296
1997.269861	166725.458256	37.716314
1999.117197	166917.773133	37.721332
2001.226162	167093.990362	37.726349
2002.957879	167275.164079	37.731367
2005.300015	167451.751867	37.736384
2006.948633	167640.855028	37.741402
2008.660554	167829.150029	37.746420
2010.931138	168013.641017	37.751437
2012.727282	168198.690170	37.756455
2014.537776	168358.306970	37.761472
2016.855551	168532.975770	37.766490
2018.510641	168690.132598	37.771508
2020.843130	168838.265789	37.776525
2022.249510	169026.183982	37.781543
2024.460258	169187.351639	37.786560
2026.289258	169353.983980	37.791578
2028.127032	169534.707766	37.796596
2030.317459	169706.307232	37.801613
2032.508886	169880.799327	37.806631
2034.137937	170067.152515	37.811648
2036.253549	170253.442093	37.816666
2038.146648	170435.708849	37.821684
2040.084216	170610.307958	37.826701
2042.134946	170817.983989	37.831719
2044.235325	171002.072483	37.836736
2046.299567	171194.970777	37.841754
2048.227863	171386.293316	37.846772
2050.778595	171572.545588	37.851789
2052.630158	171775.184406	37.856807
2054.675299	171954.339063	37.861824
2057.100871	172150.153044	37.866842
2058.879706	172342.531471	37.871860
2061.274917	172524.791788	37.876877
2063.717143	172733.481465	37.881895
2065.986024	172915.814377	37.886912
2068.377800	173123.994031	37.891930
2070.344260	173310.841986	37.896948
2072.608384	173496.210142	37.901965
2074.617871	173673.919456	37.906983
2076.386527	173847.278563	37.912000
2078.817234	174036.555340	37.917018
2080.586594	174217.641495	37.922036
2082.783367	174402.123873	37.927053
2085.023150	174590.507505	37.932071
2087.371643	174765.326279	37.937088
2089.218101	174954.750829	37.942106
2091.420498	175148.344236	37.947124
2093.842244	175323.648569	37.952141
2095.745869	175507.434049	37.957159
2097.840665	175690.746021	37.962176
2100.274207	175873.852851	37.967194
2102.032411	176055.507229	37.972212
2104.517411	176231.033808	37.977229
2106.661503	176415.736726	37.982247
2108.808553	176593.525906	37.987264
2110.814192	176769.841286	37.992282
2112.661230	176963.880306	37.997300
2114.804162	177132.512795	38.002317
2116.695011	177324.313726	38.007335
2118.715803	177508.330669	38.012352
2121.207438	177686.729628	38.017370
2122.877571	177884.721252	38.022388
2125.341745	178056.960367	38.027405
2127.206345	178235.905195	38.032423
2129.281588	178410.440370	38.037440
2131.187451	178569.245847	38.042458
2133.014967	178739.203613	38.047476
2135.170145	178900.990330	38.052493
2137.282185	179068.481061	38.057511
2139.274036	179242.728446	38.062528
2140.901622	179419.089673	38.067546
2143.004467	179598.167469	38.072564
2145.296336	179777.647414	38.077581
2147.187346	179969.891844	38.082599
2149.346402	180152.287184	38.087616
2151.854684	180339.322315	38.092634
2153.609651	180541.893215	38.097652
2155.947061	180731.659636	38.102669
2158.005453	180918.743294	38.107687
2160.539391	181118.795393	38.112704
2162.711964	181314.642625	38.117722
2164.956323	181505.670645	38.122740
2167.409957	181680.780994	38.127757
2169.556183	181886.239791	38.132775
2171.756120	182085.029804	38.137792
2173.898766	182260.559782	38.142810
2176.235153	182461.144280	38.147828
2178.454945	182653.665785	38.152845
2180.764847	182842.240476	38.157863
2182.664262	183051.169765	38.162880
2185.277859	183238.276903	38.167898
2187.414107	183433.175135	38.172916
2189.902932	183632.142083	38.177933
2192.140676	183824.577067	38.182951
2194.283565	184015.809825	38.187968
2196.488628	184196.895287	38.192986
2198.494800	184410.572346	38.198004
2200.853189	184585.963210	38.203021
2203.066061	184798.949536	38.208039
2205.312433	184996.704866	38.213056
2207.780305	185179.402205	38.218074
2209.763314	185380.525507	38.223092
2212.244930	185571.774668	38.228109
2214.118274	185765.532042	38.233127
2215.957550	185974.852593	38.238144
2218.520764	186178.945538	38.243162
2220.522462	186386.859107	38.248180
2223.096555	186577.095402	38.253197
2225.415131	186786.724368	38.258215
2227.314238	186994.644291	38.263232
2229.699949	187192.920088	38.268250
2231.947954	187390.152655	38.273268
2234.105901	187592.565033	38.278285
2236.371953	187793.692188	38.283303
2238.323941	188007.635911	38.288320
2240.975153	188206.051624	38.293338
2242.897521	188411.448981	38.298356
2245.395089	188619.332084	38.303373
2247.663433	188819.156262	38.308391
2249.978663	189002.781392	38.313408
2251.799056	189179.874184	38.318426
2253.511160	189361.718231	38.323444
2255.965221	189543.699130	38.328461
2258.089827	189733.118681	38.333479
2259.973281	189921.295516	38.338496
2262.290486	190111.599743	38.343514
2264.357368	190318.289627	38.348532
2266.516677	190512.617968	38.353549
2268.800886	190722.587348	38.358567
2270.846239	190925.323848	38.363584
2273.458833	191125.357001	38.368602
2275.348746	191338.957661	38.373620
2277.946528	191552.231283	38.378637
2280.151539	191768.563147	38.383655
2282.007858	191982.159289	38.388672
2284.511127	192186.909783	38.393690
2286.950337	192422.167583	38.398708
2289.069601	192639.138777	38.403725
2291.508114	192862.507361	38.408743
2293.456223	193096.691391	38.413760
2296.017916	193317.872339	38.418778
2298.375531	193545.698761	38.423796
2300.890736	193772.701697	38.428813
2302.915235	194000.341895	38.433831
2305.353107	194247.500410	38.438848
2307.535258	194466.804881	38.443866
2310.145498	194703.290199	38.448884
2312.455485	194942.019880	38.453901
2315.140758	195177.074078	38.458919
2317.426568	195403.993878	38.463936
2319.646142	195634.796179	38.468954
2321.809052	195871.167523	38.473972
2324.401257	196110.505256	38.478989
2326.977888	196330.542174	38.484007
2328.987695	196574.848115	38.489024
2331.835652	196804.363034	38.494042
2334.082807	197039.228757	38.499060
2336.314999	197267.548771	38.504077
2338.646298	197499.623664	38.509095
2341.058220	197741.041008	38.514112
2343.461896	197980.696546	38.519130
2345.609911	198220.317560	38.524148
2348.209356	198445.677960	38.529165
2350.816382	198688.287217	38.534183
2352.709503	198924.321796	38.539200
2355.240024	199150.914623	38.544218
2357.486508	199405.489987	38.549236
2359.902626	199639.845560	38.554253
2362.287212	199877.811907	38.559271
2364.634495	200130.623144	38.564288
2366.704083	200364.389487	38.569306
2369.234769	200607.349593	38.574324
2371.562699	200839.211173	38.579341
2374.204675	201068.218795	38.584359
2376.043192	201299.042933	38.589376
2378.786752	201506.369167	38.594394
2380.774243	201720.314963	38.599412
2383.027915	201949.108582	38.604429
2385.525373	202160.652384	38.609447
2387.406545	202378.819075	38.614464
2389.983909	202599.034142	38.619482
2392.047054	202839.450725	38.624500
2394.273269	203067.148982	38.629517
2396.751499	203297.562721	38.634535
2398.862748	203554.374833	38.639552
2401.268989	203786.185591	38.644570
2403.697182	204042.137288	38.649588
2405.952487	204284.027444	38.654605
2408.290260	204534.397734	38.659623
2410.756896	204791.514541	38.664640
2413.312540	205036.622609	38.669658
2415.364434	205304.635395	38.674676
2418.032617	205557.623515	38.679693
2420.812850	205816.688157	38.684711
2423.134882	206080.726534	38.689728
2425.731232	206338.083540	38.694746
2428.072544	206593.616042	38.699764
2430.669881	206855.862463	38.704781
2433.305586	207118.649828	38.709799
2435.546228	207391.656543	38.714816
2438.329031	207652.391841	38.719834
2440.902297	207914.646756	38.724852
2442.956210	208180.285737	38.729869
2445.580701	208442.369805	38.734887
2448.085499	208702.607856	38.739904
2450.780418	208970.357595	38.744922
2453.321251	209241.611322	38.749940
2456.044995	209493.287114	38.754957
2458.553093	209764.421394	38.759975
2461.103306	210022.321994	38.764992
2463.935008	210284.000268	38.770010
2466.106652	210546.406319	38.775028
2468.686389	210795.964762	38.780045
2471.233251	211049.896566	38.785063
2473.896540	211317.674175	38.790080
2476.544638	211568.646723	38.795098
2479.023047	211834.868909	38.800116
2481.193416	212085.881129	38.805133
2483.952974	212333.449353	38.810151
2486.399872	212598.994162	38.815168
2488.864228	212852.501894	38.820186
2491.375367	213103.172082	38.825204
2493.705804	213372.648775	38.830221
2496.098493	213617.715534	38.835239
2498.514637	213892.170205	38.840256
2501.166467	214141.374762	38.845274
2503.758156	214420.044217	38.850292
2506.050158	214667.022521	38.855309
2508.922136	214920.943397	38.860327
2510.902247	215165.370297	38.865344
2513.290238	215386.233040	38.870362
2515.555273	215643.769644	38.875380
2517.510073	215884.914871	38.880397
2520.287397	216112.980489	38.885415
2522.362508	216364.684280	38.890432
2524.755018	216603.350398	38.895450
2527.238138	216867.598788	38.900468
2529.655797	217126.932366	38.905485
2532.206353	217391.451389	38.910503
2534.145788	217662.505370	38.915520
2536.831023	217919.603005	38.920538
2539.411689	218199.229173	38.925556
2541.505633	218480.266718	38.930573
2544.606239	218755.800559	38.935591
2546.710939	219044.380448	38.940608
2549.552495	219323.931600	38.945626
2552.624681	219624.727170	38.950644
2555.090476	219892.963710	38.955661
2557.494353	220179.596190	38.960679
2560.217503	220476.070144	38.965696
2563.026649	220763.377110	38.970714
2565.537322	221048.154981	38.975732
2567.761050	221354.716880	38.980749
2571.081414	221624.576509	38.985767
2573.272843	221970.240631	38.990784
2575.391334	222268.607819	38.995802
2578.627004	222565.377061	39.000820
2581.251782	222862.447408	39.005837
2584.055040	223154.386257	39.010855
2586.338928	223457.036282	39.015872
2589.243445	223736.759010	39.020890
2592.044211	224032.739361	39.025908
2594.652041	224336.560427	39.030925
2597.255913	224623.368419	39.035943
2599.585971	224923.832768	39.040960
2602.472857	225210.750403	39.045978
2605.277859	225505.745136	39.050996
2607.850544	225805.183902	39.056013
2610.903307	226088.218222	39.061031
2613.086222	226392.927028	39.066048
2615.764020	226691.260354	39.071066
2618.758160	226977.887848	39.076084
2621.311140	227267.024249	39.081101
2624.077590	227552.394581	39.086119
2626.891226	227847.510585	39.091136
2629.179969	228142.736167	39.096154
2631.987611	228422.134742	39.101172
2634.730689	228717.671272	39.106189
2637.748162	229007.070145	39.111207
2639.960147	229300.280114	39.116224
2642.635032	229584.528843	39.121242
2645.027291	229869.432789	39.126260
2647.814897	230174.719589	39.131277
2650.610690	230451.459831	39.136295
2652.771379	230727.209461	39.141312
2655.260897	230994.907716	39.146330
2657.989994	231253.070219	39.151348
2660.037974	231520.585990	39.156365
2662.841118	231780.973218	39.161383
2665.167631	232061.170546	39.166400
2667.551490	232336.965849	39.171418
2670.504760	232618.030669	39.176436
2672.500809	232915.832682	39.181453
2675.285625	233198.779945	39.186471
2678.076053	233500.166025	39.191488
2680.463012	233800.982011	39.196506
2683.362572	234097.679440	39.201524
2686.026885	234398.072365	39.206541
2688.914663	234700.945230	39.211559
2691.546401	235012.774375	39.216576
2693.869878	235318.354529	39.221594
2696.676323	235630.437301	39.226612
2698.934670	235951.776715	39.231629
2702.092295	236264.694751	39.236647
2705.044762	236584.402281	39.241664
2707.243519	236908.192384	39.246682
2710.163499	237234.205939	39.251700
2712.554564	237567.822353	39.256717
2715.923173	237891.379369	39.261735
2718.253163	238227.750601	39.266752
2721.257297	238564.066894	39.271770
2724.355492	238886.653745	39.276788
2726.793675	239228.624139	39.281805
2729.707325	239554.290075	39.286823
2731.995624	239886.126467	39.291840
2735.279295	240225.451429	39.296858
2738.140883	240560.323121	39.301876
2740.738567	240905.930838	39.306893
2743.690828	241226.058280	39.311911
2746.445332	241561.025998	39.316928
2749.153200	241904.892001	39.321946
2752.300984	242231.468148	39.326964
2754.878126	242567.406555	39.331981
2757.602583	242900.782542	39.336999
2760.632556	243239.343469	39.342016
2763.302539	243571.713871	39.347034
2766.376705	243907.881977	39.352052
2769.274720	244249.235135	39.357069
2771.987950	244570.094922	39.362087
2775.233254	244907.864153	39.367104
2777.831895	245237.557684	39.372122
2781.011227	245559.895494	39.377140
2783.491152	245892.784511	39.382157
2786.410199	246225.985808	39.387175
2788.888149	246552.653559	39.392192
2791.618787	246886.521299	39.397210
2794.468999	247208.051454	39.402228
2797.517613	247546.569558	39.407245
2800.422518	247857.932123	39.412263
2802.828694	248166.885025	39.417280
2805.184533	248455.297036	39.422298
2808.317367	248754.102646	39.427316
2810.422193	249059.828365	39.432333
2812.964339	249358.703304	39.437351
2815.856360	249677.615863	39.442368
2818.478965	249980.391062	39.447386
2821.375880	250303.952568	39.452404
2823.503503	250630.481512	39.457421
2826.311103	250957.640081	39.462439
2829.272986	251291.811108	39.467456
2831.719372	251626.318449	39.472474
2834.611815	251967.741282	39.477492
2837.098150	252316.900422	39.482509
2840.140567	252664.473504	39.487527
2843.046458	253023.321899	39.492544
2845.717441	253373.063531	39.497562
2848.723847	253731.745006	39.502580
2851.526651	254094.523730	39.507597
2854.509858	254457.299990	39.512615
2857.439386	254819.602798	39.517632
2860.234225	255180.987728	39.522650
2863.239648	255544.803983	39.527668
2866.332895	255918.234426	39.532685
2869.113757	256278.582043	39.537703
2872.346525	256659.078959	39.542720
2875.397408	257024.490957	39.547738
2878.328787	257391.599047	39.552756
2881.221558	257759.145697	39.557773
2884.387173	258120.527751	39.562791
2887.568260	258482.974826	39.567808
2890.355305	258860.929591	39.572826
2893.728864	259210.925456	39.577844
2896.533407	259578.209479	39.582861
2899.499068	259932.894215	39.587879
2902.593877	260287.152550	39.592896
2905.488385	260651.654966	39.597914
2908.360899	261013.925914	39.602932
2911.374173	261381.331818	39.607949
2914.520013	261738.149637	39.612967
2917.661369	262091.869457	39.617984
2920.325868	262455.699327	39.623002
2923.630783	262809.546511	39.628020
2926.117656	263169.315467	39.633037
2929.321042	263527.701244	39.638055
2931.878418	263888.425138	39.643072
2934.833060	264254.167123	39.648090
2937.952127	264613.634307	39.653108
2940.550036	264980.779864	39.658125
2943.500967	265341.188878	39.663143
2946.726031	265708.058026	39.668160
2949.301143	266074.979587	39.673178
2952.530329	266438.952773	39.678196
2955.504294	266808.682379	39.683213
2958.229331	267163.971868	39.688231
2961.277995	267500.818464	39.693248
2963.597916	267834.960889	39.698266
2966.699400	268152.670928	39.703284
2969.132993	268502.469586	39.708301
2972.120439	268847.354167	39.713319
2975.367235	269190.521280	39.718336
2977.631415	269536.917922	39.723354
2980.946884	269880.760426	39.728372
2983.593675	270234.641647	39.733389
2986.547620	270594.495011	39.738407
2989.290852	270962.028301	39.743424
2992.287200	271325.431743	39.748442
2995.650288	271692.206735	39.753460
2998.300971	272073.828584	39.758477
3001.192650	272444.666785	39.763495
3004.175462	272825.245577	39.768512
3006.752679	273217.675848	39.773530
3009.781450	273602.058073	39.778548
3012.903663	274003.344258	39.783565
3015.819257	274397.296225	39.788583
3019.026454	274800.880791	39.793600
3021.739080	275205.839247	39.798618
3025.158209	275595.926517	39.803636
3028.200584	276012.950241	39.808653
3031.249366	276419.125679	39.813671
3034.592704	276838.032389	39.818688
3037.329369	277252.157614	39.823706
3040.666072	277658.820820	39.828724
3043.781507	278079.668663	39.833741
3047.102175	278479.576928	39.838759
3050.539598	278889.932805	39.843776
3053.180013	279305.774801	39.848794
3056.374967	279706.794928	39.853812
3059.658276	280121.848974	39.858829
3062.901559	280547.578576	39.863847
3065.834868	280943.990765	39.868864
3068.959566	281365.521753	39.873882
3072.032564	281784.088490	39.878900
3075.135067	282199.398677	39.883917
3078.612540	282612.845619	39.888935
3081.670448	283020.185680	39.893952
3084.049740	283444.983242	39.898970
3087.458115	283858.897457	39.903988
3090.412508	284283.730334	39.909005
3093.987884	284701.046839	39.914023
3097.288547	285120.718121	39.919040
3100.080606	285543.187615	39.924058
3103.138990	285951.846059	39.929076
3106.246431	286372.105523	39.934093
3109.795090	286789.856017	39.939111
3112.737145	287216.008809	39.944128
3115.204698	287633.903997	39.949146
3118.746136	288051.069883	39.954164
3121.700244	288473.688195	39.959181
3124.965172	288891.582636	39.964199
3128.219738	289273.304507	39.969216
3130.883304	289661.571723	39.974234
3133.926526	290045.459880	39.979252
3136.966664	290425.359777	39.984269
3139.723162	290818.462636	39.989287
3143.218367	291212.718173	39.994304
3146.210810	291608.195789	39.999322
3149.247473	292000.693698	40.004340
3152.255766	292406.836649	40.009357
3154.792024	292807.668281	40.014375
3158.334509	293219.263092	40.019392
3161.245552	293645.868301	40.024410
3164.245799	294072.153769	40.029428
3167.422514	294506.285217	40.034445
3170.042897	294929.276016	40.039463
3173.529763	295363.737694	40.044480
3176.484836	295810.653451	40.049498
3179.977447	296244.197880	40.054516
3182.923332	296693.983563	40.059533
3185.918200	297144.243093	40.064551
3189.409411	297597.852293	40.069568
3192.442498	298048.103616	40.074586
3195.921753	298508.189944	40.079604
3199.122790	298974.999760	40.084621
3202.665976	299433.778083	40.089639
3205.948803	299890.386434	40.094656
3209.028919	300350.226211	40.099674
3212.383134	300802.985145	40.104692
3215.865074	301259.202603	40.109709
3218.795090	301734.938070	40.114727
3222.650722	302183.193942	40.119744
3225.966759	302652.337419	40.124762
3229.525017	303115.116257	40.129780
3232.847720	303578.819955	40.134797
3235.983662	304036.582513	40.139815
3239.295238	304495.458871	40.144832
3242.310390	304955.269660	40.149850
3246.126159	305409.186335	40.154868
3249.531209	305868.551405	40.159885
3252.349904	306334.179986	40.164903
3255.768224	306784.979855	40.169920
3258.931152	307254.767210	40.174938
3262.537465	307719.504281	40.179956
3265.681447	308174.355937	40.184973
3269.335002	308636.161154	40.189991
3272.456393	309084.104259	40.195008
3275.502822	309557.940023	40.200026
3278.626976	310023.252715	40.205044
3282.169659	310484.890636	40.210061
3285.125995	310943.800135	40.215079
3288.623734	311407.321078	40.220096
3291.600911	311874.402187	40.225114
3295.570757	312332.942606	40.230132
3298.863230	312793.010627	40.235149
3301.921439	313233.658124	40.240167
3305.171734	313655.630643	40.245184
3308.304542	314090.751280	40.250202
3311.512989	314507.367904	40.255220
3314.578351	314935.130103	40.260237
3317.598403	315354.490800	40.265255
3320.841120	315775.998835	40.270272
3324.108554	316218.531011	40.275290
3327.146248	316664.831111	40.280308
3330.190413	317115.242674	40.285325
3333.420822	317563.413101	40.290343
3336.769896	318007.600636	40.295360
3339.522612	318478.294067	40.300378
3342.814546	318947.807800	40.305396
3346.486343	319419.824265	40.310413
3349.544058	319906.259552	40.315431
3353.071217	320383.729015	40.320448
3356.038081	320866.237015	40.325466
3359.415944	321358.074302	40.330484
3363.062916	321842.069511	40.335501
3366.452599	322336.363001	40.340519
3370.089605	322826.347975	40.345536
3373.365327	323331.041002	40.350554
3376.869857	323819.949227	40.355572
3380.543757	324318.503744	40.360589
3384.024535	324828.006074	40.365607
3387.468239	325319.759516	40.370624
3391.281753	325821.914520	40.375642
3394.532400	326315.216239	40.380660
3398.185738	326813.682687	40.385677
3401.429544	327317.619940	40.390695
3405.306663	327808.781752	40.395712
3408.549650	328314.236443	40.400730
3412.272672	328811.942756	40.405748
3416.045387	329302.324380	40.410765
3419.206072	329807.960012	40.415783
3422.676172	330316.412863	40.420800
3426.024445	330818.101330	40.425818
3429.842326	331307.218401	40.430836
3433.495844	331801.919399	40.435853
3436.679496	332309.210285	40.440871
3440.761591	332792.815994	40.445888
3443.431085	333301.400033	40.450906
3446.827713	333801.612758	40.455924
3450.511260	334296.139369	40.460941
3453.795799	334805.707148	40.465959
3457.101615	335303.892026	40.470976
3460.759152	335816.922865	40.475994
3464.196531	336322.036944	40.481012
3467.935980	336818.034607	40.486029
3471.261854	337330.979373	40.491047
3474.853057	337832.706002	40.496064
3478.599593	338335.394493	40.501082
3481.926556	338842.715813	40.506100
3485.616326	339337.508906	40.511117
3488.815880	339828.393184	40.516122
3491.985287	340276.671759	40.521127
3494.986390	340690.380158	40.526132
3497.761794	341047.509506	40.531136
3500.285429	341354.784981	40.536141
3502.609885	341623.195481	40.541146
3504.880841	341832.278333	40.546151
3506.632365	342018.482503	40.551156
3508.199789	342158.667873	40.556160
3509.750093	342251.128361	40.561165
3511.098103	342320.711622	40.566170
3512.254393	342362.096071	40.571175
3513.074177	342375.457380	40.576180
3513.720221	342363.595287	40.581184
3514.304752	342329.673852	40.586189
3514.663638	342292.478979	40.591194
3515.249901	342216.888118	40.596199
3515.561490	342153.100610	40.601204
3515.495854	342055.568924	40.606208
3515.975867	341955.787178	40.611213
3515.546844	341848.894379	40.616218
3515.867936	341737.326412	40.621223
3515.730806	341630.336182	40.626228
3515.959253	341511.120553	40.631232
3515.763280	341375.502463	40.636237
3515.458572	341250.948721	40.641242
3515.440117	341119.094798	40.646247
3514.830721	340998.916072	40.651252
3514.706814	340867.485568	40.656256
3514.506645	340733.190410	40.661261
3514.467322	340613.429927	40.666266
3514.342911	340485.282426	40.671271
3514.001167	340357.016289	40.676276
3513.597922	340234.385252	40.681280
3513.541692	340101.822413	40.686285
3512.893280	340006.136076	40.691290
3513.001083	339876.346935	40.696295
3512.531534	339759.707509	40.701300
3512.361879	339656.028277	40.706304
3512.217336	339532.565863	40.711309
3511.932415	339442.294181	40.716314
3511.766412	339334.973687	40.721319
3511.543595	339228.705681	40.726324
3511.323835	339130.404687	40.731328
3511.092138	339029.407110	40.736333
3510.820805	338941.856353	40.741338
3510.719166	338840.939743	40.746343
3510.314858	338754.580726	40.751348
3510.064405	338673.186647	40.756352
3509.893312	338588.699741	40.761357
3509.418484	338524.167380	40.766362
3509.169261	338435.874217	40.771367
3509.198475	338367.214500	40.776372
3508.946165	338305.014164	40.781376
3509.084817	338231.143949	40.786381
3508.767666	338169.564682	40.791386
3509.058258	338105.445483	40.796391
3508.836512	338038.505204	40.801396
3508.259667	337981.803501	40.806400
3508.284332	337919.406274	40.811405
3507.663836	337858.307426	40.816410
3508.018512	337804.156677	40.821415
3507.648872	337754.091581	40.826420
3507.633360	337706.592470	40.831424
3507.775685	337654.868068	40.836429
3507.582832	337603.985762	40.841434
3507.321224	337564.696962	40.846439
3507.056763	337517.135245	40.851444
3506.744727	337479.305384	40.856448
3506.896422	337436.056331	40.861453
3506.816185	337399.080756	40.866458
3506.749517	337362.332124	40.871463
3506.944458	337322.207310	40.876468
3506.648109	337276.356048	40.881472
3507.151381	337233.865891	40.886477
3506.727149	337206.058038	40.891482
3506.681863	337167.142109	40.896487
3506.732987	337128.898244	40.901492
3506.443701	337100.687164	40.906496
3506.670841	337062.160869	40.911501
3506.216751	337033.619421	40.916506
3506.601458	336988.754928	40.921511
3506.221358	336958.954375	40.926516
3505.834481	336930.605911	40.931520
3506.445988	336902.354168	40.936525
3506.221579	336877.874870	40.941530
3506.195964	336834.347974	40.946535
3505.980605	336809.383543	40.951540
3505.884243	336779.207116	40.956544
3505.990665	336756.686554	40.961549
3505.612628	336729.431247	40.966554
3505.866161	336700.039543	40.971559
3505.839888	336682.071237	40.976564
3505.516351	336658.523973	40.981568
3505.808147	336641.065422	40.986573
3505.520098	336614.763199	40.991578
3505.690966	336585.919106	40.996583
3505.571451	336568.780128	41.001588
3505.426636	336538.331228	41.006592
3505.817143	336515.536563	41.011597
3505.512387	336500.692511	41.016602
3505.444838	336478.504840	41.021607
3505.341861	336455.202662	41.026612
3505.327452	336436.265054	41.031616
3505.309006	336404.548729	41.036621
3505.158657	336393.193291	41.041626
3505.285379	336375.811681	41.046631
3505.562359	336360.646520	41.051636
3505.138042	336346.203187	41.056640
3505.445288	336318.559351	41.061645
3505.023327	336307.475950	41.066650
3505.176775	336282.351189	41.071655
3505.067805	336264.981354	41.076660
3505.074677	336261.034462	41.081664
3505.054512	336237.591831	41.086669
3505.128311	336226.710068	41.091674
3505.215279	336213.509640	41.096679
3505.372246	336189.351653	41.101684
3505.064144	336177.690177	41.106688
3504.947865	336156.910237	41.111693
3504.960240	336143.365190	41.116698
3504.963064	336123.508318	41.121703
3505.201353	336105.243464	41.126708
3505.240590	336093.196122	41.131712
3505.119828	336081.097702	41.136717
3504.725490	336067.209624	41.141722
3505.140491	336046.345660	41.146727
3505.158704	336027.733721	41.151732
3504.842285	336014.189713	41.156736
3504.762904	335993.556632	41.161741
3504.593551	335991.470488	41.166746
3504.817009	335970.484040	41.171751
3504.841880	335960.679165	41.176756
3504.632185	335951.700540	41.181760
3504.690464	335939.141019	41.186765
3504.797913	335919.471204	41.191770
3504.608394	335914.562513	41.196775
3504.726399	335909.757948	41.201780
3504.791045	335897.630183	41.206784
3504.704018	335888.581243	41.211789
3504.529278	335886.470491	41.216794
3504.871825	335873.356877	41.221799
3504.868179	335851.337098	41.226804
3504.744448	335840.588328	41.231808
3504.768459	335827.677806	41.236813
3504.782544	335812.172225	41.241818
3504.841271	335807.122453	41.246823
3504.535466	335785.685019	41.251828
3504.674955	335790.525292	41.256832
3504.666460	335765.145913	41.261837
3504.245514	335766.383505	41.266842
3504.407715	335747.519613	41.271847
3504.641612	335739.056345	41.276852
3504.441026	335742.728442	41.281856
3504.720971	335716.768846	41.286861
3504.513670	335719.907406	41.291866
3504.521596	335703.028089	41.296871
3504.813700	335698.323272	41.301876
3504.511848	335684.751437	41.306880
3504.767168	335668.393059	41.311885
3504.574722	335660.990011	41.316890
3504.781933	335640.056943	41.321895
3504.602201	335624.098275	41.326900
3504.528855	335627.699348	41.331904
3504.625410	335615.719232	41.336909
3504.434749	335607.501266	41.341914
3504.380815	335600.585458	41.346919
3504.366720	335584.320566	41.351924
3504.307805	335578.652945	41.356928
3504.306344	335567.808432	41.361933
3504.255524	335553.025854	41.366938
3504.198912	335555.835113	41.371943
3504.313909	335555.587836	41.376948
3504.164328	335534.252911	41.381952
3504.426151	335534.491567	41.386957
3504.588862	335535.636892	41.391962
3504.745236	335527.491341	41.396967
3504.680347	335517.649678	41.401972
3504.626177	335511.090299	41.406976
3504.667272	335489.928874	41.411981
3504.487772	335486.215058	41.416986
3504.588696	335479.580243	41.421991
3504.464668	335466.132996	41.426996
3504.450055	335455.061428	41.432000
3504.771885	335448.773546	41.437005
3504.338858	335436.826205	41.442010
3504.489137	335420.280715	41.447015
3504.469799	335411.959270	41.452020
3504.202505	335405.229916	41.457024
3504.609797	335390.374881	41.462029
3504.165440	335384.259033	41.467034
3504.449847	335376.729654	41.472039
3504.236307	335363.500196	41.477044
3504.491086	335355.517268	41.482048
3504.608958	335348.396073	41.487053
3504.368799	335337.080113	41.492058
3504.780117	335326.832195	41.497063
3504.337842	335305.594385	41.502068
3504.334905	335315.879610	41.507072
3504.547776	335296.447522	41.512077
3504.223453	335296.142409	41.517082
3504.324785	335285.739832	41.522087
3504.184461	335272.422410	41.527092
3504.509703	335253.405319	41.532096
3504.649643	335253.154097	41.537101
3504.429467	335244.940754	41.542106
3504.499182	335228.280668	41.547111
3504.357084	335221.429674	41.552116
3504.085378	335213.199016	41.557120
3504.639621	335209.343730	41.562125
3504.338164	335201.474177	41.567130
3504.638516	335189.309024	41.572135
3504.822215	335173.140051	41.577140
3504.700583	335169.289782	41.582144
3504.670016	335149.641564	41.587149
3504.320583	335147.074716	41.592154
3504.225940	335133.189983	41.597159
3504.412670	335121.246439	41.602164
3504.068078	335120.791786	41.607168
3504.417389	335115.059591	41.612173
3504.102558	335110.450683	41.617178
3504.297125	335087.890174	41.622183
3504.487185	335087.274626	41.627188
3504.518960	335074.566392	41.632192
3504.339539	335073.881967	41.637197
3504.029103	335058.834838	41.642202
3504.321537	335039.771960	41.647207
3504.590202	335046.017478	41.652212
3504.262368	335034.027979	41.657216
3504.438948	335020.456749	41.662221
3504.400862	335010.941722	41.667226
3504.237942	334999.740783	41.672231
3504.209033	334997.734236	41.677236
3504.314392	334986.898200	41.682240
3504.332883	334969.126023	41.687245
3504.142152	334976.131524	41.692250
3504.634771	334964.877860	41.697255
3504.488442	334951.841356	41.702260
3504.044040	334945.165412	41.707264
3504.447331	334936.369778	41.712269
3504.162455	334921.013088	41.717274
3504.088897	334921.788457	41.722279
3504.173163	334914.570700	41.727284
3504.221749	334894.655322	41.732288
3504.302790	334887.285327	41.737293
3504.173264	334894.764851	41.742298
3504.159601	334869.029552	41.747303
3504.227868	334862.119809	41.752308
3504.182872	334875.670302	41.757312
3504.447773	334858.648323	41.762317
3504.419395	334847.018769	41.767322
3504.366964	334841.604637	41.772327
3504.214161	334827.041685	41.777332
3504.293005	334824.890811	41.782336
3504.561768	334809.573859	41.787341
3504.251132	334804.276916	41.792346
3504.127887	334800.350509	41.797351
3504.179588	334782.012969	41.802356
3504.188152	334764.165936	41.807360
3504.495946	334760.247756	41.812365
3504.599805	334769.319677	41.817370
3504.389609	334753.543824	41.822375
3504.186093	334755.358040	41.827380
3504.134447	334737.418688	41.832384
3504.318332	334727.893988	41.837389
3504.247873	334727.752400	41.842394
3504.472668	334710.405776	41.847399
3504.265396	334704.685164	41.852404
3504.151075	334699.204432	41.857408
3504.322275	334689.376242	41.862413
3504.070081	334687.481358	41.867418
3504.177623	334678.376040	41.872423
3504.297418	334667.079437	41.877428
3503.985626	334653.458054	41.882432
3504.511113	334647.825256	41.887437
3504.027703	334653.018659	41.892442
3503.599464	334625.006717	41.897447
3504.002857	334620.462435	41.902452
3503.879277	334629.010265	41.907456
3503.850099	334629.931367	41.912461
3504.023258	334637.286695	41.917466
3503.717759	334617.910907	41.922471
3504.276355	334609.345254	41.927476
3504.193473	334614.169850	41.932480
3504.271952	334609.422358	41.937485
3503.913624	334602.070877	41.942490
3503.950354	334589.412686	41.947495
3504.179062	334585.659744	41.952500
3503.997797	334589.659796	41.957504
3504.256706	334582.974461	41.962509
3504.051950	334576.591544	41.967514
3504.350140	334573.998665	41.972519
3504.324945	334551.880045	41.977524
3504.197189	334539.044187	41.982528
3504.545506	334530.409938	41.987533
3504.257023	334529.335428	41.992538
3504.072798	334516.406663	41.997543
3504.212681	334507.423498	42.002548
3504.092049	334500.798157	42.007552
3504.384066	334486.775794	42.012557
3504.257350	334491.887362	42.017562
3504.222790	334472.621446	42.022567
3504.381043	334469.185128	42.027572
3503.919958	334468.265192	42.032576
3504.046018	334457.553089	42.037581
3504.038851	334442.126932	42.042586
3503.895356	334435.505199	42.047591
3504.309854	334438.698262	42.052596
3504.238144	334436.673008	42.057600
3504.127102	334404.181207	42.062605
3503.907154	334413.889890	42.067610
3504.239844	334406.887383	42.072615
3503.855235	334398.419901	42.077620
3503.865794	334395.185131	42.082624
3503.955491	334381.627511	42.087629
3503.850102	334402.290323	42.092634
3503.815207	334395.498672	42.097639
3504.193547	334397.424572	42.102644
3503.873160	334383.600834	42.107648
3504.357913	334381.742183	42.112653
3504.106948	334384.913164	42.117658
3504.176224	334361.990361	42.122663
3503.972927	334348.988207	42.127668
3503.643969	334353.189825	42.132672
3504.103128	334339.726534	42.137677
3504.163935	334341.600805	42.142682
3503.949373	334327.403918	42.147687
3504.059514	334331.994358	42.152692
3503.898029	334327.437528	42.157696
3503.916081	334317.888073	42.162701
3504.024123	334318.100128	42.167706
3503.834378	334302.830092	42.172711
3504.111171	334306.834119	42.177716
3503.909944	334312.110225	42.182720
3504.074763	334294.314742	42.187725
3503.831165	334292.622149	42.192730
3503.747282	334290.777018	42.197735
3503.783963	334287.639944	42.202740
3503.861973	334290.529803	42.207744
3504.029488	334286.913807	42.212749
3503.677144	334270.498417	42.217754
3503.999321	334256.751274	42.222759
3504.072074	334260.049288	42.227764
3503.703555	334269.399614	42.232768
3503.873527	334278.435690	42.237773
3504.071966	334268.272185	42.242778
3503.793583	334251.896013	42.247783
3503.845187	334250.080377	42.252788
3503.997958	334250.539939	42.257792
3503.920877	334250.984923	42.262797
3504.017408	334242.186781	42.267802
3503.976422	334216.913798	42.272807
3504.036248	334225.941836	42.277812
3503.909372	334235.075762	42.282816
3504.305403	334222.793483	42.287821
3503.945436	334207.219386	42.292826
3503.956831	334200.827721	42.297831
3504.039405	334204.989746	42.302836
3503.772198	334198.132971	42.307840
3503.703886	334178.363156	42.312845
3503.910459	334179.807063	42.317850
3503.710692	334175.943633	42.322855
3504.330131	334181.624622	42.327860
3503.800370	334185.883452	42.332864
3504.034444	334168.331565	42.337869
3503.758626	334170.742753	42.342874
3503.900533	334159.951726	42.347879
3503.869015	334162.527955	42.352884
3503.863548	334165.940169	42.357888
3504.176560	334150.336042	42.362893
3504.031750	334143.816320	42.367898
3504.135636	334141.508720	42.372903
3504.271112	334139.832568	42.377908
3503.832628	334124.194493	42.382912
3504.250942	334114.047120	42.387917
3503.919125	334115.652516	42.392922
3504.030939	334111.408874	42.397927
3503.833397	334095.987279	42.402932
3503.737400	334092.973002	42.407936
3503.874734	334082.182686	42.412941
3504.085743	334091.390503	42.417946
3504.048831	334090.174385	42.422951
3504.104260	334076.265715	42.427956
3503.851329	334067.930122	42.432960
3504.021389	334064.237339	42.437965
3504.261124	334072.116815	42.442970
3504.164938	334058.053906	42.447975
3504.092006	334040.245028	42.452980
3504.056628	334036.075567	42.457984
3504.454174	334023.385689	42.462989
3503.897018	334028.845375	42.467994
3503.843925	334018.136069	42.472999
3504.067224	334017.540714	42.478004
3503.781039	334016.134882	42.483008
3503.853685	333998.812135	42.488013
3503.731486	333995.191010	42.493018
3504.041418	333999.368020	42.498023
3504.086539	333994.778506	42.503028
3503.796169	334004.752957	42.508032
3503.809318	333987.515986	42.513037
3503.904358	333982.867664	42.518042
3503.806840	333971.452557	42.523047
3504.124654	333973.133460	42.528052
3504.015100	333978.064148	42.533056
3504.334160	333958.334862	42.538061
3504.109820	333951.394912	42.543066
3503.976979	333940.596371	42.548071
3503.976890	333947.826414	42.553076
3503.831012	333934.738732	42.558080
3504.158422	333916.841075	42.563085
3503.964149	333921.657871	42.568090
3503.811629	333919.263510	42.573095
3503.914268	333916.956099	42.578100
3503.521289	333904.798499	42.583104
3503.859639	333894.256411	42.588109
3503.607286	333893.863540	42.593114
3503.707001	333895.986250	42.598119
3504.033816	333901.662607	42.603124
3503.739880	333903.185645	42.608128
3504.029849	333906.118384	42.613133
3503.405265	333890.306014	42.618138
3503.648726	333876.163916	42.623143
3503.636259	333879.475420	42.628148
3503.534387	333882.215528	42.633152
3503.624940	333884.365144	42.638157
3503.807366	333890.904436	42.643162
3503.590032	333895.393928	42.648167
3503.556697	333893.795374	42.653172
3503.542482	333902.275087	42.658176
3504.079844	333900.688143	42.663181
3503.863356	333881.221705	42.668186
3503.924281	333868.432268	42.673191
3503.993262	333876.186014	42.678196
3504.018584	333873.254380	42.683200
3504.351677	333865.640767	42.688205
3504.240479	333851.020118	42.693210
3504.085990	333847.200428	42.698215
3503.813419	333846.581632	42.703220
3503.782055	333838.847429	42.708224
3503.847824	333818.088918	42.713229
3503.320815	333823.849347	42.718234
3503.780874	333812.167862	42.723239
3504.056704	333820.779937	42.728244
3503.773424	333822.530413	42.733248
3504.133349	333815.829035	42.738253
3503.555391	333811.872626	42.743258
3503.925169	333794.019156	42.748263
3503.803801	333792.918215	42.753268
3503.754170	333805.935035	42.758272
3504.134661	333799.561357	42.763277
3504.236417	333787.885596	42.768282
3504.051812	333772.385511	42.773287
3504.057470	333768.387751	42.778292
3504.097011	333762.806247	42.783296
3503.938960	333764.384180	42.788301
3503.668233	333747.115655	42.793306
3503.815922	333737.011011	42.798311
3503.920800	333745.166422	42.803316
3503.791045	333749.845740	42.808321
3503.922285	333745.140764	42.813325
3503.623952	333733.171834	42.818330
3503.575690	333718.923076	42.823335
3503.700326	333721.703755	42.828340
3503.837312	333720.256476	42.833345
3503.882843	333721.343983	42.838349
3504.257012	333725.179902	42.843354
3504.035175	333719.486970	42.848359
3504.163122	333702.766396	42.853364
3503.916676	333704.129183	42.858369
3504.140712	333695.489021	42.863373
3504.255635	333686.535154	42.868378
3504.311873	333675.808512	42.873383
3504.109259	333672.480120	42.878388
3504.043237	333663.096614	42.883393
3503.909236	333644.609927	42.888397
3503.778385	333649.060305	42.893402
3503.723359	333646.319569	42.898407
3504.132745	333645.287466	42.903412
3503.655225	333655.418843	42.908417
3504.006313	333637.542830	42.913421
3503.843619	333620.333568	42.918426
3503.775089	333615.380127	42.923431
3504.117677	333614.791369	42.928436
3503.861151	333628.910162	42.933441
3504.046629	333610.042007	42.938445
3503.907080	333607.518295	42.943450
3504.185364	333595.407268	42.948455
3503.986938	333599.588295	42.953460
3503.820324	333591.468120	42.958465
3503.928144	333575.641724	42.963469
3503.471771	333571.997033	42.968474
3503.587619	333571.087709	42.973479
3503.844236	333571.021700	42.978484
3503.762984	333575.897025	42.983489
3504.251126	333567.011431	42.988493
3503.639365	333567.668236	42.993498
3503.489884	333556.261276	42.998503
3503.864902	333552.510607	43.003508
3503.676931	333547.779708	43.008513
3503.680299	333550.401360	43.013517
3503.728987	333551.742951	43.018522
3504.105932	333550.741433	43.023527
3504.239080	333551.331392	43.028532
3503.911270	333541.200060	43.033537
3504.124240	333519.094377	43.038541
3503.642676	333529.684654	43.043546
3503.635507	333536.304868	43.048551
3504.021546	333523.413056	43.053556
3503.788656	333509.906266	43.058561
3503.911184	333500.136519	43.063565
3503.590656	333502.274760	43.068570
3503.675324	333494.445802	43.073575
3503.884494	333500.140791	43.078580
3503.557965	333504.443906	43.083585
3503.911898	333491.073463	43.088589
3503.565457	333482.090676	43.093594
3503.592629	333471.317682	43.098599
3504.038828	333470.559795	43.103604
3503.820216	333467.539417	43.108609
3503.896438	333466.840020	43.113613
3503.683807	333483.726820	43.118618
3503.811536	333464.816840	43.123623
3503.928459	333452.833130	43.128628
3503.768123	333457.873714	43.133633
3503.969907	333449.567993	43.138637
3503.391000	333465.316178	43.143642
3503.755560	333466.073217	43.148647
3504.100701	333466.655120	43.153652
3503.586216	333450.290627	43.158657
3503.944863	333431.038637	43.163661
3503.901803	333429.059740	43.168666
3504.113601	333425.105746	43.173671
3503.889845	333434.916999	43.178676
3503.615614	333412.251855	43.183681
3504.102577	333398.223914	43.188685
3503.657230	333408.732109	43.193690
3503.881251	333404.521602	43.198695
3504.136834	333407.281592	43.203700
3503.858202	333400.732041	43.208705
3503.890726	333380.589648	43.213709
3503.759812	333375.060520	43.218714
3503.912001	333380.178992	43.223719
3504.068605	333381.758105	43.228724
3503.614642	333387.685227	43.233729
3503.751718	333370.988590	43.238733
3503.543241	333359.540009	43.243738
3503.416283	333363.760667	43.248743
3503.644983	333353.719535	43.253748
3503.634784	333356.114217	43.258753
3503.849964	333355.851094	43.263757
3503.763819	333366.251594	43.268762
3503.863759	333359.845854	43.273767
3503.916827	333362.739694	43.278772
3503.479309	333354.458655	43.283777
3503.928737	333338.730950	43.288781
3503.846430	333332.608599	43.293786
3503.605388	333339.011225	43.298791
3503.668988	333338.542944	43.303796
3503.760414	333339.368622	43.308801
3503.913075	333341.253856	43.313805
3503.856157	333345.157946	43.318810
3503.694085	333329.526911	43.323815
3503.690416	333315.729266	43.328820
3503.676524	333325.609189	43.333825
3503.791266	333316.298892	43.338829
3503.894528	333322.494340	43.343834
3503.628466	333320.830732	43.348839
3504.092183	333321.241143	43.353844
3503.849212	333306.004762	43.358849
3503.856407	333288.972225	43.363853
3503.607909	333291.557330	43.368858
3503.516441	333285.461882	43.373863
3503.550465	333291.388240	43.378868
3503.492290	333299.085777	43.383873
3503.510265	333305.396542	43.388877
3503.538128	333300.504215	43.393882
3503.527976	333300.938624	43.398887
3503.644510	333309.066784	43.403892
3503.681796	333305.013082	43.408897
3503.762553	333290.514719	43.413901
3503.425482	333290.007947	43.418906
3503.500601	333285.311812	43.423911
3503.537810	333282.632855	43.428916
3503.860446	333288.971831	43.433921
3503.984190	333283.657016	43.438925
3503.798596	333291.069202	43.443930
3503.757545	333299.273192	43.448935
3503.631027	333292.750499	43.453940
3503.762686	333275.443703	43.458945
3504.027978	333259.083181	43.463949
3503.643755	333260.111346	43.468954
3503.793459	333263.957318	43.473959
3503.833519	333262.627184	43.478964
3503.893459	333269.593227	43.483969
3504.011948	333245.160256	43.488973
3503.854992	333237.522216	43.493978
3503.896944	333227.026887	43.498983
3504.078374	333223.739592	43.503988
3503.907046	333238.506903	43.508993
3504.029257	333207.174200	43.513997
3503.911779	333203.959617	43.519002
3503.759274	333206.580465	43.524007
3504.135183	333201.480360	43.529012
3503.622179	333204.285491	43.534017
3503.616948	333178.370030	43.539021
3503.665484	333182.461123	43.544026
3503.361605	333174.489890	43.549031
3503.245348	333187.059112	43.554036
3503.473625	333187.735867	43.559041
3503.731320	333187.924268	43.564045
3503.426185	333193.191427	43.569050
3503.321170	333188.727427	43.574055
3503.389215	333192.229900	43.579060
3503.613608	333189.343140	43.584065
3503.902894	333199.607938	43.589069
3503.923119	333195.582385	43.594074
3504.027802	333195.845892	43.599079
3503.925608	333180.179900	43.604084
3503.820757	333173.577396	43.609089
3504.039556	333162.163067	43.614093
3503.795974	333168.006032	43.619098
3503.885246	333170.206788	43.624103
3503.800983	333148.784431	43.629108
3503.805488	333143.386624	43.634113
3503.847211	333139.535876	43.639117
3503.728165	333141.845940	43.644122
3503.782097	333147.209086	43.649127
3503.904040	333140.214312	43.654132
3503.500482	333150.384984	43.659137
3503.856630	333129.249410	43.664141
3503.774717	333116.864290	43.669146
3503.653886	333105.503644	43.674151
3503.915211	333114.678177	43.679156
3503.682129	333112.169233	43.684161
3504.086197	333115.414923	43.689165
3503.948039	333111.414404	43.694170
3504.032471	333094.496901	43.699175
3503.837735	333091.829146	43.704180
3503.971647	333092.520820	43.709185
3503.737227	333083.851228	43.714189
3503.810017	333088.982273	43.719194
3503.351306	333069.986692	43.724199
3503.655016	333062.173974	43.729204
3503.612847	333061.365998	43.734209
3503.664603	333056.800832	43.739213
3503.620318	333054.160208	43.744218
3503.709835	333061.656215	43.749223
3503.935071	333064.421016	43.754228
3503.587269	333060.020849	43.759233
3503.970816	333063.498909	43.764237
3503.897487	333045.664384	43.769242
3503.747410	333033.901021	43.774247
3503.969302	333029.767202	43.779252
3503.487573	333033.051099	43.784257
3503.824612	333036.460138	43.789261
3503.525550	333036.303769	43.794266
3503.592175	333043.217861	43.799271
3503.662280	333039.820866	43.804276
3503.524109	333035.209350	43.809281
3503.844885	333012.246348	43.814285
3503.580713	333014.019281	43.819290
3503.619787	333011.034521	43.824295
3503.669480	333008.964574	43.829300
3503.520602	333016.167319	43.834305
3503.862153	333011.479962	43.839309
3503.531275	333026.781703	43.844314
3503.901888	333020.256767	43.849319
3504.063535	333006.636592	43.854324
3503.542631	333005.038723	43.859329
3503.954411	332987.152951	43.864333
3503.909321	333007.144729	43.869338
3503.830710	333000.461686	43.874343
3503.813493	333005.301470	43.879348
3503.650167	332985.902754	43.884353
3503.796575	332961.363439	43.889357
3503.671814	332965.405567	43.894362
3503.699685	332973.725989	43.899367
3503.834612	332964.692495	43.904372
3503.862131	332973.547594	43.909377
3503.876724	332971.126782	43.914381
3503.872173	332959.925937	43.919386
3503.753988	332948.335724	43.924391
3503.765609	332945.380759	43.929396
3503.746661	332940.877680	43.934401
3503.958245	332934.097838	43.939405
3503.914263	332942.964245	43.944410
3503.637040	332929.871683	43.949415
3503.652993	332918.463925	43.954420
3503.572175	332918.273053	43.959425
3503.653138	332917.318319	43.964429
3503.454790	332917.604275	43.969434
3503.760615	332914.144552	43.974439
3503.965436	332913.832149	43.979444
3503.868127	332922.885196	43.984449
3503.831304	332915.864583	43.989453
3503.470851	332911.109993	43.994458
3503.449723	332909.280363	43.999463
3503.984577	332902.042082	44.004468
3503.772720	332903.272125	44.009473
3503.813902	332898.352207	44.014477
3503.736550	332894.800309	44.019482
3503.595823	332901.619904	44.024487
3503.784325	332895.174664	44.029492
3503.607910	332890.569185	44.034497
3503.695382	332871.563578	44.039501
3503.560593	332878.204030	44.044506
3503.409598	332876.649511	44.049511
3503.956108	332869.383926	44.054516
3503.510723	332883.099935	44.059521
3503.512830	332875.665833	44.064525
3503.552893	332878.739956	44.069530
3503.522008	332886.025892	44.074535
3503.549109	332875.991106	44.079540
3503.628402	332883.234167	44.084545
3503.862912	332876.985317	44.089549
3503.211178	332868.305297	44.094554
3503.051044	332875.560752	44.099559
3503.907514	332888.001706	44.104564
3503.640009	332871.521660	44.109569
3503.573911	332866.033161	44.114573
3503.549690	332859.443340	44.119578
3503.425763	332855.924262	44.124583
3503.806389	332865.716421	44.129588
3503.450173	332870.915304	44.134593
3503.733116	332860.560030	44.139597
3503.573428	332875.325576	44.144602
3503.652346	332874.320248	44.149607
3503.833258	332871.185768	44.154612
3504.021373	332867.846484	44.159617
3504.052436	332847.398673	44.164621
3504.049466	332843.249476	44.169626
3503.920381	332839.985794	44.174631
3503.863662	332839.180116	44.179636
3503.926199	332828.986972	44.184641
3503.959281	332812.408477	44.189645
3503.529760	332814.054805	44.194650
3503.693995	332805.958611	44.199655
3503.614689	332805.996624	44.204660
3503.431719	332818.881956	44.209665
3503.491042	332809.147564	44.214669
3503.515107	332812.529717	44.219674
3503.675518	332816.526770	44.224679
3503.894695	332815.244686	44.229684
3503.476983	332802.148852	44.234689
3503.651136	332780.914655	44.239693
3503.486600	332789.800139	44.244698
3503.357907	332785.314400	44.249703
3503.896314	332788.437034	44.254708
3503.836181	332788.395642	44.259713
3504.042749	332785.435309	44.264717
3503.726232	332787.165606	44.269722
3503.723570	332776.880929	44.274727
3503.712301	332763.262586	44.279732
3503.630064	332763.962976	44.284737
3503.907156	332758.063798	44.289741
3503.495529	332769.126838	44.294746
3503.542764	332771.410627	44.299751
3503.607517	332760.377002	44.304756
3503.653311	332766.734333	44.309761
3503.835950	332761.613834	44.314765
3503.670120	332772.459808	44.319770
3504.004618	332748.858097	44.324775
3503.884767	332732.863840	44.329780
3503.372566	332740.124051	44.334785
3503.713434	332728.283023	44.339789
3503.373089	332742.186119	44.344794
3503.794265	332735.882288	44.349799
3503.935945	332738.660312	44.354804
3503.629712	332751.259644	44.359809
3503.727977	332729.757388	44.364813
3503.415056	332726.039058	44.369818
3503.551209	332715.146887	44.374823
3503.566244	332711.427626	44.379828
3503.522174	332721.057822	44.384833
3504.189989	332713.263879	44.389837
3503.760264	332722.776835	44.394842
3503.667231	332724.089929	44.399847
3504.039027	332719.550521	44.404852
3503.984525	332705.939001	44.409857
3503.929603	332692.964001	44.414861
3503.722771	332686.581241	44.419866
3503.825434	332685.495782	44.424871
3503.929476	332694.287902	44.429876
3503.452880	332684.129053	44.434881
3503.427834	332669.341790	44.439885
3503.362769	332663.547613	44.444890
3503.413583	332662.928600	44.449895
3503.538888	332657.766241	44.454900
3503.468418	332654.493285	44.459905
3503.378020	332664.410852	44.464909
3503.589723	332664.377402	44.469914
3503.629665	332663.225483	44.474919
3503.608081	332669.644391	44.479924
3503.546837	332678.844517	44.484929
3503.684990	332664.922492	44.489933
3503.788865	332668.928491	44.494938
3503.523626	332673.578383	44.499943
3503.560569	332675.711052	44.504948
3503.750685	332676.266554	44.509953
3503.840476	332668.233029	44.514957
3503.692943	332661.433560	44.519962
3503.533583	332636.025975	44.524967
3503.673272	332635.520202	44.529972
3503.556559	332644.372686	44.534977
3503.515348	332642.113433	44.539981
3503.853743	332641.576247	44.544986
3503.866267	332652.368584	44.549991
3503.903798	332656.130490	44.554996
3503.836912	332644.277535	44.560001
3503.980590	332622.615319	44.565005
3504.087179	332621.249197	44.570010
3503.954587	332610.704996	44.575015
3504.069116	332610.534158	44.580020
3503.555988	332600.304697	44.585025
3503.890532	332579.783374	44.590029
3503.668318	332575.923405	44.595034
3503.459746	332575.956395	44.600039
3503.938155	332581.812560	44.605044
3503.602157	332589.757761	44.610049
3503.685326	332582.310813	44.615053
3503.423835	332593.248312	44.620058
3503.404059	332593.149623	44.625063
3503.684358	332587.428132	44.630068
3503.333855	332577.045667	44.635073
3503.707800	332559.802227	44.640077
3503.854190	332564.259760	44.645082
3503.475798	332561.493728	44.650087
3503.802540	332562.867754	44.655092
3503.706600	332571.105964	44.660097
3503.781111	332562.922094	44.665101
3503.498092	332570.578880	44.670106
3503.260412	332571.889386	44.675111
3503.643889	332568.544662	44.680116
3503.312913	332576.438154	44.685121
3503.408217	332583.984213	44.690125
3503.408949	332583.042158	44.695130
3503.482007	332587.765865	44.700135
3503.580641	332580.189182	44.705140
3503.428595	332595.971908	44.710145
3503.687989	332586.027649	44.715149
3503.683913	332573.477380	44.720154
3503.626999	332564.779663	44.725159
3503.791448	332559.509276	44.730164
3503.622634	332554.724365	44.735169
3503.592697	332552.386953	44.740173
3503.504660	332557.467087	44.745178
3503.669842	332554.233247	44.750183
3503.702621	332555.119122	44.755188
3503.759885	332564.249611	44.760193
3504.191242	332555.118286	44.765197
3503.457806	332537.973532	44.770202
3503.368716	332541.500878	44.775207
3503.915910	332533.827818	44.780212
3503.740735	332537.419690	44.785217
3503.670690	332544.839144	44.790221
3503.618181	332536.395310	44.795226
3503.657548	332548.710916	44.800231
3504.113854	332543.343472	44.805236
3503.656003	332529.973892	44.810241
3503.658459	332508.155759	44.815245
3503.671270	332513.474536	44.820250
3503.535346	332511.128420	44.825255
3503.971658	332508.971880	44.830260
3503.803283	332510.449639	44.835265
3503.895732	332514.762952	44.840269
3503.633912	332489.040556	44.845274
3503.499456	332478.802130	44.850279
3503.613323	332475.856440	44.855284
3503.366000	332484.220425	44.860289
3503.492527	332477.835861	44.865293
3503.754925	332487.901346	44.870298
3503.280867	332488.383641	44.875303
3503.734929	332482.634672	44.880308
3503.720291	332487.346791	44.885313
3503.713121	332484.522069	44.890317
3503.674172	332487.023159	44.895322
3503.823704	332486.719495	44.900327
3503.966712	332458.514549	44.905332
3503.409829	332466.087350	44.910337
3503.775808	332451.467350	44.915341
3503.948782	332454.062229	44.920346
3503.937663	332459.741210	44.925351
3503.606411	332449.788475	44.930356
3503.851824	332461.027731	44.935361
3503.624338	332440.595220	44.940365
3503.637891	332434.712221	44.945370
3503.356480	332431.116185	44.950375
3503.502126	332425.365053	44.955380
3503.409469	332434.926593	44.960385
3503.579192	332426.702196	44.965389
3503.478377	332432.879068	44.970394
3503.600933	332438.180501	44.975399
3503.678876	332438.651905	44.980404
3503.592414	332441.975173	44.985409
3503.853334	332439.795442	44.990413
3503.733418	332445.313416	44.995418
3503.622151	332440.875817	45.000423
3503.992584	332419.508649	45.005428
3503.375559	332412.401503	45.010433
3503.593667	332407.071705	45.015437
3503.727018	332414.280809	45.020442
3503.693396	332418.155809	45.025447
3503.498223	332418.670390	45.030452
3503.558072	332421.995988	45.035457
3503.646095	332412.231547	45.040461
3503.681650	332422.765694	45.045466
3503.723158	332423.650191	45.050471
3503.918063	332404.983894	45.055476
3503.652936	332398.126615	45.060481
3503.825872	332389.443456	45.065485
3503.849889	332385.340883	45.070490
3503.319758	332395.837172	45.075495
3503.569169	332389.051298	45.080500
3503.737713	332395.211049	45.085505
3503.944475	332388.177334	45.090509
3503.984861	332380.686213	45.095514
3503.832329	332365.715375	45.100519
3503.956258	332360.120421	45.105524
3503.292788	332367.964666	45.110529
3503.648371	332360.907422	45.115533
3503.412846	332360.842840	45.120538
3503.398997	332366.878677	45.125543
3503.496231	332364.572071	45.130548
3503.418573	332374.080331	45.135553
3503.668715	332367.447090	45.140557
3503.523202	332371.441615	45.145562
3503.762947	332367.966853	45.150567
3503.979491	332355.559877	45.155572
3503.729868	332347.885474	45.160577
3503.959678	332343.088448	45.165581
3503.841769	332334.858595	45.170586
3504.066485	332333.371961	45.175591
3504.064947	332316.977032	45.180596
3503.808918	332302.633544	45.185601
3503.685209	332298.783446	45.190605
3503.628500	332306.149899	45.195610
3503.803921	332298.739255	45.200615
3503.785289	332294.388835	45.205620
3503.422266	332302.974800	45.210625
3503.726838	332302.672083	45.215629
3503.628935	332289.321930	45.220634
3503.377615	332272.253644	45.225639
3503.816499	332263.681177	45.230644
3503.711283	332271.488095	45.235649
3503.523602	332268.208192	45.240653
3503.482175	332270.684223	45.245658
3503.680394	332270.296486	45.250663
3504.013886	332267.112400	45.255668
3503.349107	332274.422236	45.260673
3503.584730	332275.301506	45.265677
3503.847038	332279.206105	45.270682
3503.471639	332266.867235	45.275687
3503.690845	332242.239790	45.280692
3503.775145	332256.381348	45.285697
3503.991857	332243.719742	45.290701
3503.672471	332249.167431	45.295706
3503.646229	332248.789721	45.300711
3503.904362	332240.754993	45.305716
3503.714736	332242.312493	45.310721
3503.684158	332222.052457	45.315725
3503.617817	332227.638353	45.320730
3503.814443	332222.108270	45.325735
3503.724031	332221.969831	45.330740
3503.679160	332227.144998	45.335745
3503.710584	332221.895616	45.340749
3503.452253	332225.526108	45.345754
3503.593624	332229.398912	45.350759
3503.547119	332223.194431	45.355764
3503.548581	332239.411219	45.360769
3503.812648	332229.313422	45.365773
3503.658742	332206.348830	45.370778
3503.657777	332196.012884	45.375783
3503.638107	332190.084201	45.380788
3503.582793	332195.337396	45.385793
3503.534005	332185.034468	45.390797
3503.803391	332192.069338	45.395802
3504.003769	332192.190428	45.400807
3503.600163	332187.951780	45.405812
3503.810528	332169.792146	45.410817
3503.984890	332163.985536	45.415821
3503.990036	332162.024441	45.420826
3503.603124	332160.201702	45.425831
3503.611115	332165.266683	45.430836
3503.245711	332176.831674	45.435841
3503.547086	332164.996797	45.440845
3503.731422	332169.270147	45.445850
3503.523995	332162.531015	45.450855
3503.430589	332165.040725	45.455860
3503.486482	332168.061459	45.460865
3503.757820	332162.061309	45.465869
3503.443534	332151.596681	45.470874
3503.669205	332141.734068	45.475879
3503.534161	332132.386731	45.480884
3503.674220	332143.286274	45.485889
3503.534052	332139.184185	45.490893
3503.860592	332140.863753	45.495898
3503.546170	332145.088660	45.500903
3503.799339	332155.282943	45.505908
3503.437568	332151.266805	45.510913
3503.550870	332152.954625	45.515917
3503.641069	332155.638976	45.520922
3503.608368	332144.264245	45.525927
3503.579016	332136.631373	45.530932
3503.348012	332141.683221	45.535937
3503.267307	332132.505502	45.540941
3503.387961	332136.279752	45.545946
3503.081035	332129.149013	45.550951
3503.437786	332131.027473	45.555956
3503.552339	332134.599020	45.560961
3503.754465	332129.551771	45.565965
3503.335554	332138.426633	45.570970
3503.238287	332134.190469	45.575975
3503.637862	332130.384927	45.580980
3503.430864	332145.667271	45.585985
3503.661122	332143.339628	45.590989
3503.507788	332143.440261	45.595994
3503.508534	332152.554279	45.600999
3503.732886	332145.950554	45.606004
3503.337108	332151.894037	45.611009
3503.681098	332145.398690	45.616013
3503.422784	332160.969186	45.621018
3503.557518	332148.447815	45.626023
3504.219514	332147.579425	45.631028
3503.591020	332147.144174	45.636033
3503.754459	332121.990877	45.641037
3503.594466	332120.845100	45.646042
3503.447568	332113.714519	45.651047
3503.776839	332109.996466	45.656052
3503.619397	332127.027612	45.661057
3503.653385	332114.114827	45.666061
3503.384969	332126.097287	45.671066
3503.401283	332127.367647	45.676071
3503.449188	332121.708318	45.681076
3503.489883	332132.012569	45.686081
3503.419714	332133.322060	45.691085
3503.633292	332136.114199	45.696090
3503.516050	332132.543112	45.701095
3503.315098	332136.775540	45.706100
3503.191822	332135.420290	45.711105
3503.222230	332127.930720	45.716109
3503.411300	332140.146355	45.721114
3503.483388	332131.224524	45.726119
3503.656326	332129.466028	45.731124
3503.820968	332146.573543	45.736129
3503.603231	332130.263668	45.741133
3503.626721	332118.141755	45.746138
3503.546923	332110.109520	45.751143
3503.556063	332105.245529	45.756148
3503.196430	332111.845221	45.761153
3503.516385	332103.978915	45.766157
3503.378418	332108.506888	45.771162
3503.378049	332110.492722	45.776167
3503.726827	332113.747199	45.781172
3503.718307	332104.150730	45.786177
3503.529630	332117.495342	45.791181
3503.837443	332117.319404	45.796186
3503.648040	332115.389065	45.801191
3503.848623	332117.088546	45.806196
3503.946420	332103.223709	45.811201
3503.996345	332084.427498	45.816205
3503.804260	332092.859171	45.821210
3503.793561	332083.415794	45.826215
3504.080969	332076.369300	45.831220
3503.784454	332085.581237	45.836225
3503.758962	332063.283677	45.841229
3503.712011	332061.534483	45.846234
3503.733243	332046.536109	45.851239
3503.690280	332057.006347	45.856244
3503.327198	332057.496558	45.861249
3503.874256	332050.027137	45.866253
3503.983571	332058.385707	45.871258
3503.669528	332048.812072	45.876263
3504.152461	332023.251814	45.881268
3504.104413	332023.794055	45.886273
3503.910467	332007.964103	45.891277
3503.662593	332019.052286	45.896282
3503.807269	332011.621015	45.901287
3503.872427	331994.935426	45.906292
3503.854957	331993.232487	45.911297
3503.786727	331985.936705	45.916301
3503.716544	331991.675977	45.921306
3503.513258	331994.406732	45.926311
3503.433876	331998.339905	45.931316
3503.350515	331995.705419	45.936321
3503.885763	331993.533223	45.941325
3503.598619	331996.735487	45.946330
3503.617862	331978.453269	45.951335
3503.369635	331966.145160	45.956340
3503.171902	331964.241591	45.961345
3503.497806	331956.807122	45.966349
3503.840962	331957.873064	45.971354
3503.408100	331959.545398	45.976359
3503.507083	331964.035921	45.981364
3503.580248	331960.409265	45.986369
3503.638489	331960.501909	45.991373
3503.459101	331972.368486	45.996378
3503.533854	331970.116339	46.001383
3503.768596	331956.586243	46.006388
3503.008393	331973.076253	46.011393
3503.505931	331965.691027	46.016397
3503.561968	331964.714763	46.021402
3503.343540	331968.975422	46.026407
3503.719519	331970.061633	46.031412
3503.360187	331971.798718	46.036417
3503.480906	331968.546422	46.041421
3503.745807	331974.818267	46.046426
3503.771477	331971.988334	46.051431
3503.694264	331955.630745	46.056436
3503.450361	331948.108147	46.061441
3503.465680	331934.510902	46.066445
3503.789232	331942.606490	46.071450
3503.703026	331949.952185	46.076455
3503.893629	331947.248927	46.081460
3503.836520	331945.144917	46.086465
3503.858839	331946.134288	46.091469
3503.382439	331955.832933	46.096474
3503.284268	331942.890093	46.101479
3503.764912	331940.319192	46.106484
3503.495844	331933.767994	46.111489
3503.884372	331913.950785	46.116493
3504.051858	331916.673844	46.121498
3503.938937	331910.963548	46.126503
3504.049958	331906.032521	46.131508
3503.814479	331904.007625	46.136513
3503.846487	331886.538038	46.141517
3503.626759	331883.950564	46.146522
3503.844438	331880.530185	46.151527
3503.864648	331868.968837	46.156532
3503.552815	331881.238245	46.161537
3503.680789	331882.109079	46.166541
3503.718907	331873.014377	46.171546
3503.678316	331860.367922	46.176551
3503.302491	331847.418043	46.181556
3503.321225	331845.021996	46.186561
3503.601595	331836.041743	46.191565
3503.180147	331851.281675	46.196570
3503.283371	331853.123847	46.201575
3503.518302	331838.677192	46.206580
3503.556507	331848.345414	46.211585
3503.475823	331841.026128	46.216589
3503.752700	331844.266525	46.221594
3503.519132	331859.502213	46.226599
3503.735778	331853.867104	46.231604
3503.663582	331852.580149	46.236609
3503.642528	331854.416510	46.241613
3503.773953	331856.356057	46.246618
3503.462601	331861.598837	46.251623
3504.049642	331852.748313	46.256628
3503.429209	331848.289338	46.261633
3503.597862	331838.537531	46.266637
3503.569752	331834.061289	46.271642
3503.597814	331838.944910	46.276647
3503.604687	331829.956976	46.281652
3503.517481	331837.557425	46.286657
3503.585833	331825.479288	46.291661
3503.380474	331827.573913	46.296666
3503.562146	331834.622684	46.301671
3503.390286	331823.117151	46.306676
3503.352920	331837.074357	46.311681
3503.528127	331829.358197	46.316685
3503.760984	331826.240918	46.321690
3503.437511	331829.067055	46.326695
3503.624236	331831.608865	46.331700
3503.180600	331835.752384	46.336705
3503.602487	331834.667364	46.341709
3503.528775	331833.787985	46.346714
3503.602202	331837.951595	46.351719
3503.905567	331829.400501	46.356724
3503.378146	331813.750517	46.361729
3503.438865	331799.382313	46.366733
3503.564717	331792.132205	46.371738
3503.627993	331802.229265	46.376743
3503.848305	331797.968334	46.381748
3503.700698	331799.468282	46.386753
3503.971743	331792.653475	46.391757
3503.890477	331804.479108	46.396762
3503.497486	331789.826210	46.401767
3503.896392	331774.437111	46.406772
3503.706792	331774.696230	46.411777
3503.723371	331773.675284	46.416781
3503.434523	331775.681275	46.421786
3503.383862	331778.922538	46.426791
3503.384009	331780.755549	46.431796
3503.527775	331782.260352	46.436801
3503.654313	331781.527525	46.441805
3503.806689	331778.804846	46.446810
3503.653588	331786.110215	46.451815
3503.960647	331779.518840	46.456820
3503.712166	331760.667886	46.461825
3503.763752	331746.912121	46.466829
3503.505016	331744.228975	46.471834
3503.566234	331744.219314	46.476839
3503.522885	331745.830075	46.481844
3503.360092	331755.224582	46.486849
3503.599959	331748.414699	46.491853
3503.601950	331748.083440	46.496858
3503.402735	331746.536520	46.501863
3503.800405	331748.764941	46.506868
3503.797627	331760.069003	46.511873
3503.903774	331750.556193	46.516877
3503.851320	331741.399417	46.521882
3503.592606	331735.533946	46.526887
3503.646964	331732.063003	46.531892
3503.512532	331740.052807	46.536897
3503.625028	331728.476847	46.541901
3503.794667	331732.345208	46.546906
3503.396878	331740.707608	46.551911
3503.768432	331739.681460	46.556916
3504.085304	331735.227050	46.561921
3503.731928	331714.712400	46.566925
3503.588301	331705.773702	46.571930
3503.505722	331712.660592	46.576935
3503.908921	331697.067130	46.581940
3503.484076	331708.005128	46.586945
3503.598813	331701.851488	46.591949
3503.893398	331705.343678	46.596954
3503.705547	331709.879562	46.601959
3503.881457	331682.203742	46.606964
3503.729582	331678.205311	46.611969
3503.659046	331672.513754	46.616973
3503.648819	331669.282147	46.621978
3503.632831	331667.222545	46.626983
3503.924899	331664.452319	46.631988
3503.616380	331673.589830	46.636993
3503.708414	331663.417317	46.641997
3503.835179	331649.115018	46.647002
3503.582191	331647.169259	46.652007
3503.506019	331646.239350	46.657012
3503.418991	331649.791872	46.662017
3503.482215	331641.075051	46.667021
3503.601848	331645.765998	46.672026
3503.302865	331644.234848	46.677031
3503.336615	331639.239643	46.682036
3503.219350	331653.336808	46.687041
3503.293637	331648.640698	46.692045
3503.501160	331649.269832	46.697050
3503.374438	331655.654534	46.702055
3503.599501	331654.269665	46.707060
3503.421586	331657.607428	46.712065
3503.532726	331644.936948	46.717069
3503.527590	331662.962469	46.722074
3503.401551	331659.494584	46.727079
3503.744185	331661.349829	46.732084
3503.385802	331662.908561	46.737089
3503.143149	331659.790073	46.742093
3503.454722	331663.992420	46.747098
3503.543201	331660.465163	46.752103
3503.655997	331667.957636	46.757108
3503.097193	331667.740491	46.762113
3503.119601	331665.445692	46.767117
3503.075310	331668.482285	46.772122
3503.222405	331671.870501	46.777127
3503.754750	331670.946226	46.782132
3503.472280	331671.474612	46.787137
3503.946444	331673.054478	46.792141
3503.946383	331671.425154	46.797146
3503.767687	331672.166263	46.802151
3503.559307	331651.755966	46.807156
3503.313749	331645.481070	46.812161
3503.392459	331635.972583	46.817165
3503.452033	331645.382868	46.822170
3503.237955	331650.610284	46.827175
3503.549901	331644.170876	46.832180
3503.144283	331649.912287	46.837185
3503.538847	331646.769436	46.842189
3503.340620	331653.801908	46.847194
3503.197332	331648.758315	46.852199
3503.336848	331663.629560	46.857204
3503.583060	331679.324067	46.862209
3503.621298	331665.010307	46.867213
3503.789982	331660.248358	46.872218
3503.128152	331659.945667	46.877223
3503.780773	331646.196699	46.882228
3503.244965	331660.258196	46.887233
3503.345726	331657.645507	46.892237
3503.546547	331660.872477	46.897242
3503.408927	331658.577518	46.902247
3503.368174	331654.994316	46.907252
3503.193232	331656.345837	46.912257
3503.501368	331655.049669	46.917261
3503.579103	331661.503883	46.922266
3503.370021	331670.498381	46.927271
3503.775284	331656.813979	46.932276
3503.452263	331661.473070	46.937281
3503.572009	331657.177112	46.942285
3503.527590	331664.185267	46.947290
3503.810165	331658.794306	46.952295
3503.890571	331651.755037	46.957300
3503.874909	331664.945086	46.962305
3503.368982	331640.661202	46.967309
3503.856367	331632.284661	46.972314
3503.261203	331633.626241	46.977319
3503.555516	331630.601072	46.982324
3503.158610	331636.366566	46.987329
3503.806894	331634.227407	46.992333
3503.528530	331639.872325	46.997338
3503.478514	331633.948393	47.002343
3503.636818	331632.319492	47.007348
3503.413670	331638.693981	47.012353
3503.442781	331643.246487	47.017357
3503.563719	331637.142778	47.022362
3503.557926	331637.271004	47.027367
3503.897202	331636.657296	47.032372
3503.709725	331639.996571	47.037377
3503.650435	331631.120907	47.042381
3503.631215	331613.175639	47.047386
3503.349117	331608.103071	47.052391
3503.817411	331607.239838	47.057396
3503.530517	331617.621410	47.062401
3503.972192	331609.226635	47.067405
3503.647551	331612.562137	47.072410
3503.544500	331612.680280	47.077415
3503.996433	331607.007955	47.082420
3503.893882	331606.998726	47.087425
3503.764675	331583.138980	47.092429
3503.860687	331582.054557	47.097434
3503.604869	331580.618416	47.102439
3503.657720	331576.282111	47.107444
3503.534302	331583.328221	47.112449
3503.429056	331581.104518	47.117453
3503.990664	331583.077899	47.122458
3503.710651	331569.807320	47.127463
3503.531373	331553.796739	47.132468
3503.626311	331546.780622	47.137473
3503.400546	331544.525053	47.142477
3503.510150	331554.334778	47.147482
3503.537601	331551.326336	47.152487
3503.643044	331549.807624	47.157492
3503.590066	331549.001341	47.162497
3503.773190	331548.183190	47.167501
3504.042177	331555.192726	47.172506
3503.406261	331555.929742	47.177511
3503.694351	331553.516562	47.182516
3503.495318	331561.771184	47.187521
3503.710234	331541.752194	47.192525
3503.655477	331526.638432	47.197530
3503.521713	331519.760302	47.202535
3503.887494	331516.774748	47.207540
3503.734021	331517.715540	47.212545
3503.525286	331507.921516	47.217549
3503.854044	331515.685367	47.222554
3503.486183	331519.638713	47.227559
3503.785930	331517.198230	47.232564
3503.436102	331512.721912	47.237569
3503.550846	331495.850159	47.242573
3503.233787	331494.627368	47.247578
3503.455510	331497.672830	47.252583
3504.004457	331488.599158	47.257588
3503.674658	331494.710474	47.262593
3503.663722	331493.184701	47.267597
3503.772612	331490.850766	47.272602
3503.484744	331485.702725	47.277607
3503.682301	331480.019688	47.282612
3503.514399	331487.709307	47.287617
3503.876340	331489.281459	47.292621
3503.690172	331486.230410	47.297626
3503.238991	331463.388955	47.302631
3503.613111	331459.103688	47.307636
3503.356722	331458.533230	47.312641
3503.494032	331453.445264	47.317645
3503.435465	331455.440317	47.322650
3503.456382	331452.254693	47.327655
3503.849874	331452.625301	47.332660
3503.705653	331464.740987	47.337665
3503.702309	331459.267919	47.342669
3503.837689	331464.032765	47.347674
3503.737545	331459.746098	47.352679
3503.788687	331457.370374	47.357684
3503.422311	331453.405842	47.362689
3503.421956	331436.475895	47.367693
3503.677004	331436.893848	47.372698
3503.297224	331435.604596	47.377703
3503.734960	331426.879459	47.382708
3503.094110	331431.945232	47.387713
3503.523675	331433.710364	47.392717
3503.463429	331433.210733	47.397722
3503.439720	331441.590404	47.402727
3503.644625	331436.109870	47.407732
3503.462240	331446.220358	47.412737
3503.347291	331442.954378	47.417741
3503.539191	331437.654111	47.422746
3503.588243	331444.112879	47.427751
3503.799193	331444.588720	47.432756
3503.452931	331448.564115	47.437761
3503.976504	331436.999496	47.442765
3503.835110	331444.201214	47.447770
3503.735811	331440.525422	47.452775
3503.591756	331419.010168	47.457780
3503.552653	331414.815684	47.462785
3503.530023	331411.484191	47.467789
3503.388314	331406.567625	47.472794
3503.287839	331404.674125	47.477799
3503.415826	331401.115151	47.482804
3503.339800	331415.078549	47.487809
3503.291351	331408.670637	47.492813
3503.380979	331409.700291	47.497818
3503.329976	331419.128086	47.502823
3503.826145	331410.037288	47.507828
3503.544262	331417.235760	47.512833
3503.853395	331408.760081	47.517837
3503.908118	331407.885852	47.522842
3503.644644	331412.382792	47.527847
3503.797241	331411.213045	47.532852
3503.573423	331411.044776	47.537857
3503.803249	331394.256641	47.542861
3503.683608	331393.690023	47.547866
3503.388658	331388.568554	47.552871
3503.579584	331384.745042	47.557876
3503.341687	331386.386566	47.562881
3503.262455	331395.131442	47.567885
3503.428200	331389.784390	47.572890
3503.242408	331389.941073	47.577895
3503.349408	331389.211331	47.582900
3503.332776	331393.796543	47.587905
3503.558309	331391.698751	47.592909
3503.487399	331387.203790	47.597914
3503.583307	331393.833365	47.602919
3503.749589	331390.191960	47.607924
3503.372256	331405.348635	47.612929
3503.087795	331400.709224	47.617933
3503.501043	331400.745746	47.622938
3503.511237	331406.879696	47.627943
3503.781010	331396.322625	47.632948
3503.257097	331404.959589	47.637953
3503.170300	331406.271721	47.642957
3503.936179	331408.594695	47.647962
3503.123646	331411.167200	47.652967
3503.129490	331404.368823	47.657972
3503.408538	331418.174253	47.662977
3503.390241	331415.834963	47.667981
3503.729250	331408.067404	47.672986
3503.660913	331418.567204	47.677991
3503.774446	331408.569468	47.682996
3503.636886	331426.335937	47.688001
3503.610827	331406.787802	47.693005
3503.893613	331382.811941	47.698010
3503.469527	331387.563403	47.703015
3503.769622	331385.224696	47.708020
3503.630580	331379.416652	47.713025
3503.539557	331388.392521	47.718029
3503.631887	331395.404542	47.723034
3503.499836	331388.449753	47.728039
3503.562822	331378.205416	47.733044
3503.668383	331385.953649	47.738049
3503.342724	331382.644602	47.743053
3504.009013	331392.900975	47.748058
3503.747322	331375.172192	47.753063
3503.454256	331359.637813	47.758068
3503.239770	331356.667612	47.763073
3503.122179	331358.035531	47.768077
3503.391172	331354.326969	47.773082
3503.361622	331363.369499	47.778087
3503.739375	331364.913695	47.783092
3503.490321	331357.009970	47.788097
3503.453986	331363.736830	47.793101
3503.497214	331368.312580	47.798106
3503.352219	331369.633914	47.803111
3503.520221	331360.238568	47.808116
3503.494306	331360.624563	47.813121
3503.468625	331363.174511	47.818125
3503.406068	331367.436022	47.823130
3503.182794	331365.816521	47.828135
3503.736800	331365.448910	47.833140
3503.465710	331367.630315	47.838145
3503.549964	331366.725958	47.843149
3503.963322	331367.857187	47.848154
3503.685645	331374.978621	47.853159
3503.801960	331368.951997	47.858164
3503.436541	331354.090982	47.863169
3503.252716	331339.303091	47.868173
3503.363525	331347.916094	47.873178
3503.418119	331368.019859	47.878183
3503.647490	331354.439583	47.883188
3503.389670	331354.149397	47.888193
3503.353753	331341.349361	47.893197
3503.871075	331336.735943	47.898202
3503.570464	331342.078897	47.903207
3503.786310	331343.954195	47.908212
3503.801473	331345.708466	47.913217
3503.629459	331341.993247	47.918221
3503.464301	331344.896208	47.923226
3503.503158	331349.167146	47.928231
3503.718838	331343.735820	47.933236
3503.665462	331354.869732	47.938241
3503.506659	331338.066647	47.943245
3503.563994	331322.527783	47.948250
3503.229407	331323.930008	47.953255
3503.356802	331321.898646	47.958260
3503.351718	331320.321027	47.963265
3503.633214	331324.120809	47.968269
3503.516475	331322.306254	47.973274
3503.641625	331329.975019	47.978279
3504.079251	331322.675576	47.983284
3503.398478	331337.218310	47.988289
3503.649970	331334.836367	47.993293
3503.778654	331331.480949	47.998298
3503.536539	331327.547683	48.003303
3503.592714	331328.251663	48.008308
3503.642086	331331.706261	48.013313
3503.718966	331319.932197	48.018317
3503.455764	331301.974507	48.023322
3503.262949	331298.288032	48.028327
3503.513021	331296.797368	48.033332
3503.453415	331304.775390	48.038337
3503.322051	331304.337918	48.043341
3503.245223	331304.400998	48.048346
3503.612761	331292.453686	48.053351
3503.813710	331289.188676	48.058356
3503.458622	331295.202173	48.063361
3503.773575	331286.725559	48.068365
3503.553359	331289.917273	48.073370
3503.476302	331299.145533	48.078375
3503.910012	331288.333401	48.083380
3503.579840	331293.120939	48.088385
3503.246379	331295.337666	48.093389
3503.974312	331295.324439	48.098394
3503.572632	331286.910201	48.103399
3503.714083	331267.361006	48.108404
3503.524682	331274.875835	48.113409
3503.362921	331262.553937	48.118413
3503.495319	331253.571547	48.123418
3503.279493	331266.487807	48.128423
3503.702538	331263.645943	48.133428
3503.816032	331256.855993	48.138433
3503.525245	331269.987773	48.143437
3503.654958	331264.442738	48.148442
3503.530001	331268.154027	48.153447
3503.513009	331266.985629	48.158452
3503.530723	331274.951431	48.163457
3503.451839	331259.866887	48.168461
3503.853495	331269.910526	48.173466
3503.546705	331272.021202	48.178471
3503.761059	331249.074465	48.183476
3503.957191	331235.473963	48.188481
3503.534283	331221.436690	48.193485
3503.485720	331231.576969	48.198490
3503.537227	331229.277556	48.203495
3503.688303	331229.151854	48.208500
3503.367907	331234.243356	48.213505
3503.432345	331237.542824	48.218509
3503.581235	331233.802326	48.223514
3503.427026	331240.267786	48.228519
3503.619930	331236.596706	48.233524
3503.423665	331241.286702	48.238529
3503.462418	331241.306051	48.243533
3503.712893	331241.724729	48.248538
3503.678121	331231.597661	48.253543
3503.999831	331210.365135	48.258548
3503.234358	331210.282497	48.263553
3503.681503	331201.784975	48.268557
3503.798971	331199.678804	48.273562
3503.397952	331201.600708	48.278567
3503.637623	331201.384625	48.283572
3503.636590	331203.116001	48.288577
3503.642592	331202.376766	48.293581
3503.496757	331204.971173	48.298586
3503.150324	331209.837664	48.303591
3503.673013	331212.835559	48.308596
3503.543806	331217.947754	48.313601
3503.936357	331207.778586	48.318605
3503.610403	331184.764494	48.323610
3503.576828	331174.713606	48.328615
3503.845647	331164.971333	48.333620
3503.517861	331171.184194	48.338625
3503.662320	331171.008621	48.343629
3503.194775	331165.405246	48.348634
3503.351889	331176.913249	48.353639
3503.711224	331172.986726	48.358644
3503.250775	331179.933404	48.363649
3503.364825	331179.228005	48.368653
3503.454250	331183.083617	48.373658
3503.209248	331187.934074	48.378663
3503.316623	331180.966873	48.383668
3503.331625	331189.264077	48.388673
3503.520816	331186.179133	48.393677
3503.484233	331192.651461	48.398682
3503.252746	331190.880502	48.403687
3504.003933	331189.641578	48.408692
3503.654382	331197.970954	48.413697
3503.909382	331202.869658	48.418701
3503.834618	331183.430999	48.423706
3503.631484	331173.967010	48.428711
3503.618954	331164.778391	48.433716
3503.463706	331165.261210	48.438721
3503.701229	331158.222514	48.443725
3503.608503	331163.481698	48.448730
3503.573428	331168.298969	48.453735
3503.869571	331167.539323	48.458740
3503.724361	331173.596026	48.463745
3503.617045	331172.620117	48.468749
3503.642439	331166.429638	48.473754
3503.655554	331139.797700	48.478759
3503.751582	331126.722180	48.483764
3503.594764	331125.805014	48.488769
3503.835647	331118.714865	48.493773
3503.792413	331113.222619	48.498778
3503.620779	331131.605557	48.503783
3503.598559	331119.465245	48.508788
3503.463387	331128.575419	48.513793
3503.419959	331127.156610	48.518797
3503.804796	331128.674233	48.523802
3503.678556	331113.546229	48.528807
3503.540849	331095.008555	48.533812
3503.430491	331089.195954	48.538817
3503.349321	331089.539768	48.543821
3503.342116	331091.806757	48.548826
3503.148175	331092.346611	48.553831
3503.408147	331092.229153	48.558836
3503.394203	331092.740551	48.563841
3503.343964	331092.824887	48.568845
3503.294603	331088.428336	48.573850
3503.580733	331107.248087	48.578855
3503.331407	331095.347345	48.583860
3503.407069	331098.645045	48.588865
3503.478333	331090.970698	48.593869
3503.410887	331088.155451	48.598874
3503.396881	331097.577439	48.603879
3503.512473	331095.166055	48.608884
3503.420886	331094.289494	48.613889
3503.430005	331102.053003	48.618893
3503.622756	331101.131490	48.623898
3503.509510	331104.102631	48.628903
3503.688698	331104.838084	48.633908
3503.433386	331112.083303	48.638913
3503.448452	331103.908666	48.643917
3503.440311	331104.444605	48.648922
3503.228545	331104.910900	48.653927
3503.540544	331100.279010	48.658932
3503.405944	331108.523497	48.663937
3503.402768	331105.316209	48.668941
3503.585789	331107.171243	48.673946
3503.516257	331103.108846	48.678951
3503.507915	331101.429901	48.683956
3503.210511	331114.511838	48.688961
3503.408924	331107.530238	48.693965
3503.537694	331113.492714	48.698970
3503.262362	331118.322512	48.703975
3503.425884	331116.972821	48.708980
3503.556226	331116.774021	48.713985
3503.389115	331120.746569	48.718989
3503.387851	331124.718358	48.723994
3503.145790	331122.592646	48.728999
3503.718968	331124.666046	48.734004
3503.643470	331129.642463	48.739009
3503.658418	331121.646058	48.744013
3503.880936	331120.337957	48.749018
3503.651756	331109.401467	48.754023
3503.853110	331088.518898	48.759028
3503.627454	331084.837604	48.764033
3503.276406	331079.063053	48.769037
3503.089465	331079.703636	48.774042
3503.299359	331083.667503	48.779047
3503.551528	331086.555417	48.784052
3503.298627	331093.927550	48.789057
3503.583065	331085.710326	48.794061
3503.553070	331082.201770	48.799066
3503.707395	331097.936388	48.804071
3503.901328	331094.596102	48.809076
3503.891537	331105.188527	48.814081
3503.674153	331090.864149	48.819085
3503.716787	331090.042745	48.824090
3503.400622	331077.388803	48.829095
3503.773020	331059.967041	48.834100
3503.722036	331061.808153	48.839105
3503.507145	331064.489859	48.844109
3503.605059	331062.412233	48.849114
3503.457107	331068.214790	48.854119
3503.392731	331063.896988	48.859124
3503.576524	331069.621640	48.864129
3503.507218	331066.475722	48.869133
3503.476615	331059.479405	48.874138
3503.387118	331073.699585	48.879143
3503.398351	331061.884940	48.884148
3503.177381	331063.702008	48.889153
3503.324543	331064.467983	48.894157
3503.887351	331063.360674	48.899162
3503.549303	331067.487543	48.904167
3503.822751	331066.476896	48.909172
3503.588702	331074.253392	48.914177
3503.949052	331060.601438	48.919181
3503.701129	331033.348800	48.924186
3503.627124	331031.654776	48.929191
3503.846901	331027.572096	48.934196
3503.591139	331037.388734	48.939201
3503.325959	331033.764604	48.944205
3503.887576	331026.903789	48.949210
3503.728097	331035.686853	48.954215
3503.849530	331032.612614	48.959220
3503.796487	331014.901677	48.964225
3503.733474	331000.960218	48.969229
3503.617170	330994.079279	48.974234
3503.213082	330997.503744	48.979239
3503.876755	330989.048344	48.984244
3503.822140	331001.429988	48.989249
3503.539560	330996.459289	48.994253
3503.747571	330993.829621	48.999258
3503.724818	330993.833236	49.004263
3503.494151	330971.924202	49.009268
3503.229080	330971.915207	49.014273
3503.475571	330966.402605	49.019277
3503.737408	330965.979346	49.024282
3503.482106	330969.431209	49.029287
3503.697268	330966.673116	49.034292
3503.670671	330971.870942	49.039297
3503.544485	330982.481785	49.044301
3503.659695	330977.499115	49.049306
3503.435625	330968.267538	49.054311
3503.606193	330967.578660	49.059316
3503.516962	330967.541867	49.064321
3503.456785	330973.865190	49.069325
3503.675032	330974.619929	49.074330
3503.444935	330983.337786	49.079335
3503.895183	330973.286759	49.084340
3503.543786	330955.444762	49.089345
3503.284451	330953.041729	49.094349
3503.535751	330944.651516	49.099354
3503.482288	330954.028841	49.104359
3503.076843	330946.913561	49.109364
3503.283711	330957.980932	49.114369
3503.047601	330965.732306	49.119373
3503.446935	330972.364868	49.124378
3503.471121	330974.932404	49.129383
3503.654054	330977.551221	49.134388
3503.658996	330980.936483	49.139393
3503.602685	330969.438007	49.144397
3503.465437	330961.542022	49.149402
3503.303562	330963.247914	49.154407
3503.508809	330951.580791	49.159412
3503.607082	330967.222462	49.164417
3503.722274	330955.340448	49.169421
3503.714687	330955.036158	49.174426
3503.367856	330957.356844	49.179431
3503.451824	330959.405753	49.184436
3503.473152	330968.822171	49.189441
3503.655100	330967.265893	49.194445
3503.571055	330965.038819	49.199450
3503.561735	330962.952685	49.204455
3503.339099	330960.365638	49.209460
3503.436727	330970.686512	49.214465
3503.699229	330965.476885	49.219469
3503.794565	330963.526959	49.224474
3503.364365	330948.574268	49.229479
3503.612578	330929.746412	49.234484
3503.492164	330932.871446	49.239489
3503.384935	330924.206946	49.244493
3503.655160	330927.448436	49.249498
3503.411250	330930.643911	49.254503
3503.881414	330921.277117	49.259508
3503.748169	330930.616141	49.264513
3503.667052	330925.842717	49.269517
3503.750666	330930.946746	49.274522
3503.575069	330933.291280	49.279527
3503.706626	330928.102352	49.284532
3503.925171	330917.069593	49.289537
3503.638437	330902.017835	49.294541
3503.671283	330890.836217	49.299546
3503.514141	330903.004957	49.304551
3503.485727	330894.582581	49.309556
3503.547982	330893.630779	49.314561
3503.613397	330899.857877	49.319565
3503.731980	330892.914336	49.324570
3503.596856	330897.543770	49.329575
3503.748717	330899.378277	49.334580
3503.920512	330896.830707	49.339585
3503.519226	330882.153479	49.344589
3503.637752	330878.443222	49.349594
3503.285393	330865.209412	49.354599
3503.748732	330871.220851	49.359604
3503.518453	330870.137083	49.364609
3503.497497	330869.936742	49.369613
3503.507155	330862.399405	49.374618
3503.262574	330873.538159	49.379623
3503.385485	330868.223299	49.384628
3503.624885	330873.455457	49.389633
3503.611226	330864.088767	49.394637
3503.789544	330868.032179	49.399642
3503.592635	330864.880966	49.404647
3503.933709	330870.988111	49.409652
3503.502760	330858.428654	49.414657
3503.320202	330848.019391	49.419661
3503.488929	330839.413090	49.424666
3503.474723	330846.620218	49.429671
3503.578550	330840.620983	49.434676
3503.345569	330845.520480	49.439681
3503.391283	330839.403138	49.444685
3503.225682	330836.679776	49.449690
3503.207030	330839.916020	49.454695
3503.587893	330831.708983	49.459700
3503.736614	330842.709187	49.464705
3503.420642	330842.988287	49.469709
3503.703610	330835.738705	49.474714
3503.356241	330841.394593	49.479719
3503.565851	330840.750460	49.484724
3503.902534	330842.173866	49.489729
3503.386332	330837.240090	49.494733
3503.563857	330837.975809	49.499738
3503.518640	330835.488004	49.504743
3503.488518	330833.430613	49.509748
3503.405834	330843.627257	49.514753
3503.472715	330858.968407	49.519757
3503.451106	330840.234103	49.524762
3503.330259	330860.391201	49.529767
3503.696418	330850.531663	49.534772
3503.709539	330854.119308	49.539777
3503.518197	330841.903852	49.544781
3503.453916	330819.179244	49.549786
3503.483996	330813.446255	49.554791
3503.874843	330811.525983	49.559796
3503.803418	330816.629072	49.564801
3503.748715	330815.288416	49.569805
3503.588260	330818.623456	49.574810
3503.180267	330821.666664	49.579815
3503.407109	330820.103286	49.584820
3503.490523	330820.472000	49.589825
3503.502604	330820.597402	49.594829
3503.609118	330818.085609	49.599834
3503.385793	330828.508160	49.604839
3503.590473	330817.070236	49.609844
3503.379660	330816.721697	49.614849
3503.615201	330822.132681	49.619853
3503.634528	330827.654222	49.624858
3503.506124	330817.694654	49.629863
3503.748185	330798.740443	49.634868
3503.757600	330787.791644	49.639873
3504.035559	330783.725212	49.644877
3503.977329	330782.690620	49.649882
3503.742407	330801.236398	49.654887
3503.775864	330780.940381	49.659892
3503.679058	330767.818905	49.664897
3503.442792	330755.024982	49.669901
3503.510897	330752.137375	49.674906
3503.230933	330748.871993	49.679911
3503.620879	330752.094564	49.684916
3503.476898	330751.251740	49.689921
3503.245955	330752.433919	49.694925
3503.501100	330757.739973	49.699930
3503.358763	330752.517956	49.704935
3503.471317	330754.078632	49.709940
3503.781029	330757.950360	49.714945
3503.499147	330762.628463	49.719949
3503.752068	330753.041403	49.724954
3503.795142	330765.407643	49.729959
3503.693469	330753.992681	49.734964
3503.127791	330762.305357	49.739969
3503.595964	330761.620346	49.744973
3503.853621	330754.934854	49.749978
3503.380334	330757.402832	49.754983
3503.514608	330739.280331	49.759988
3503.200503	330734.212763	49.764993
3503.201668	330742.690416	49.769997
3503.514588	330758.705541	49.775002
3503.339627	330767.643837	49.780007
3503.744317	330766.790651	49.785012
3503.191664	330750.329743	49.790017
3503.568326	330734.001964	49.795021
3503.501920	330737.169386	49.800026
3503.433077	330741.508303	49.805031
3503.578029	330734.917004	49.810036
3503.519424	330737.599473	49.815041
3503.670120	330732.382046	49.820045
3503.725894	330738.101504	49.825050
3503.493492	330733.937540	49.830055
3503.909647	330741.534902	49.835060
3503.595989	330738.936779	49.840065
3503.488148	330739.386646	49.845069
3503.438615	330735.881163	49.850074
3503.259620	330744.005415	49.855079
3503.231586	330740.674746	49.860084
3503.618255	330734.376199	49.865089
3503.648025	330742.340152	49.870093
3503.676075	330741.571968	49.875098
3503.375345	330733.243543	49.880103
3503.861453	330719.240679	49.885108
3503.591756	330712.383963	49.890113
3503.574837	330707.956801	49.895117
3503.667463	330696.256525	49.900122
3503.424624	330700.979377	49.905127
3503.484629	330698.398556	49.910132
3503.306540	330707.668320	49.915137
3503.711242	330709.946580	49.920141
3503.666227	330707.153231	49.925146
3503.674410	330710.665287	49.930151
3503.996580	330704.478770	49.935156
3503.830601	330713.033769	49.940161
3503.416684	330690.415313	49.945165
3503.739797	330675.241639	49.950170
3503.481699	330676.631783	49.955175
3504.059205	330668.368181	49.960180
3503.486077	330676.631126	49.965185
3503.381952	330675.858377	49.970189
3503.667332	330675.660525	49.975194
3503.352724	330680.802068	49.980199
3503.608530	330669.992512	49.985204
3503.526429	330679.934496	49.990209
3503.574906	330682.854628	49.995213
3503.703184	330678.226298	50.000218
3503.258778	330678.500243	50.005223
3503.540037	330673.211254	50.010228
3503.612111	330666.198667	50.015233
3503.417759	330642.170703	50.020237
3503.642424	330635.719546	50.025242
3503.354579	330641.875218	50.030247
3503.533301	330630.721417	50.035252
3503.497255	330638.899458	50.040257
3503.255845	330638.937641	50.045261
3503.384730	330637.797089	50.050266
3503.592809	330641.990397	50.055271
3503.676686	330637.878263	50.060276
3503.649626	330647.556960	50.065281
3503.849687	330647.525350	50.070285
3503.739643	330644.385854	50.075290
3503.392449	330653.555065	50.080295
3503.884356	330652.178910	50.085300
3503.674047	330651.066522	50.090305
3503.193007	330637.572966	50.095309
3503.446033	330627.196645	50.100314
3503.087322	330635.552992	50.105319
3503.356751	330643.148101	50.110324
3503.510688	330650.023159	50.115329
3503.538691	330653.735756	50.120333
3503.541900	330640.853036	50.125338
3503.154866	330628.515729	50.130343
3503.782059	330626.838137	50.135348
3503.809097	330628.234123	50.140353
3503.433315	330619.001027	50.145357
3503.290046	330620.856739	50.150362
3503.405438	330625.675717	50.155367
3503.221931	330615.444784	50.160372
3503.481512	330616.549417	50.165377
3503.415374	330619.309458	50.170381
3503.399712	330620.533982	50.175386
3503.194589	330624.792615	50.180391
3503.682475	330615.652112	50.185396
3503.671889	330621.152939	50.190401
3503.199052	330623.569932	50.195405
3503.653303	330630.753940	50.200410
3503.344853	330627.824022	50.205415
3503.485322	330629.914926	50.210420
3503.674634	330628.535690	50.215425
3503.672628	330626.702980	50.220429
3503.775561	330620.169231	50.225434
3503.392355	330636.039843	50.230439
3503.671115	330628.867283	50.235444
3503.726773	330632.244543	50.240449
3503.424028	330631.375899	50.245453
3503.651057	330627.012002	50.250458
3503.525088	330603.915195	50.255463
3503.514252	330590.270918	50.260468
3503.493005	330596.180776	50.265473
3503.536294	330591.845925	50.270477
3503.782997	330594.200084	50.275482
3503.548680	330602.384015	50.280487
3503.790384	330587.121357	50.285492
3503.896520	330593.367502	50.290497
3503.504837	330591.850985	50.295501
3504.005726	330590.091524	50.300506
3503.651176	330573.879308	50.305511
3503.626517	330561.026439	50.310516
3503.652359	330571.791520	50.315521
3503.784983	330563.725533	50.320525
3503.616212	330560.137056	50.325530
3503.147526	330568.230748	50.330535
3503.529192	330566.362839	50.335540
3503.769003	330560.265708	50.340545
3503.604960	330567.776599	50.345549
3503.758415	330562.787856	50.350554
3503.485220	330571.308903	50.355559
3503.667195	330560.892888	50.360564
3503.613075	330537.886538	50.365569
3503.376724	330527.740324	50.370573
3503.868161	330524.556652	50.375578
3503.234779	330532.167204	50.380583
3503.392858	330522.060470	50.385588
3503.530116	330529.014552	50.390593
3503.287551	330532.693553	50.395597
3503.668482	330531.309481	50.400602
3503.620952	330541.144183	50.405607
3503.683965	330522.039994	50.410612
3503.511622	330539.608503	50.415617
3503.413155	330533.412094	50.420621
3503.472495	330526.172376	50.425626
3503.210667	330533.215009	50.430631
3503.172688	330534.875865	50.435636
3503.563718	330535.195949	50.440641
3503.330240	330544.627244	50.445645
3503.755147	330534.554705	50.450650
3503.468082	330531.341354	50.455655
3503.893266	330534.074643	50.460660
3503.896833	330543.952184	50.465665
3503.537696	330532.170548	50.470669
3503.670312	330510.891339	50.475674
3503.054008	330518.448275	50.480679
3503.407000	330503.346219	50.485684
3503.432054	330510.267124	50.490689
3503.301135	330510.415133	50.495693
3503.616982	330511.918217	50.500698
3503.412373	330521.064902	50.505703
3503.675412	330515.040471	50.510708
3503.752318	330513.933594	50.515713
3503.769221	330509.271942	50.520717
3503.622384	330510.237156	50.525722
3503.530019	330516.209181	50.530727
3503.679312	330485.405663	50.535732
3503.645937	330468.124288	50.540737
3503.288665	330432.105356	50.545741
3503.514155	330395.434178	50.550746
3502.674764	330361.248104	50.555751
3503.115107	330295.035865	50.560756
3502.683300	330239.068707	50.565761
3502.239718	330166.936832	50.570765
3502.123676	330086.606180	50.575770
3501.740683	330012.733355	50.580775
3501.245056	329926.886983	50.585780
3500.831187	329841.231262	50.590785
3500.485809	329741.231053	50.595789
3500.455019	329641.944756	50.600794
3499.804107	329545.149542	50.605799
3499.525198	329427.571472	50.610804
3499.062228	329316.819980	50.615809
3498.668152	329198.037711	50.620813
3498.246451	329066.326205	50.625818
3497.654604	328946.811026	50.630823
3497.030607	328814.927393	50.635828
3496.851999	328692.749611	50.640833
3496.511591	328556.899921	50.645837
3495.844439	328422.400093	50.650842
3495.312534	328278.203946	50.655847
3494.552823	328127.780435	50.660852
3494.071860	327992.053815	50.665857
3493.249426	327860.479984	50.670861
3492.881500	327695.812544	50.675866
3492.283700	327554.502449	50.680871
3491.657962	327402.630604	50.685876
3491.214655	327250.169502	50.690881
3490.347433	327095.178193	50.695885
3490.216275	326937.651494	50.700890
3489.384726	326784.665294	50.705895
3488.735372	326622.000549	50.710900
3488.253577	326464.273748	50.715905
3487.645941	326304.529701	50.720909
3487.191204	326151.151734	50.725914
3486.228830	325991.768677	50.730919
3485.778465	325829.885608	50.735924
3485.197607	325663.592706	50.740929
3484.437301	325508.505054	50.745933
3484.129620	325340.131454	50.750938
3482.899381	325172.310736	50.755943
3482.568885	325010.177948	50.760948
3481.585578	324835.341250	50.765953
3480.982883	324668.795181	50.770957
3480.816413	324502.459882	50.775962
3479.994602	324334.190982	50.780967
3479.327518	324173.917511	50.785972
3478.694979	324007.272999	50.790977
3478.218121	323837.726436	50.795981
3477.360779	323663.503906	50.800986
3476.613881	323500.772041	50.805991
3476.293005	323324.096105	50.810996
3475.661639	323165.775602	50.816001
3474.678266	322992.386392	50.821005
3474.018372	322809.932338	50.826010
3473.401469	322644.199308	50.831015
3472.824294	322479.350835	50.836020
3472.064687	322301.290863	50.841025
3471.204560	322125.690739	50.846029
3470.522521	321953.524899	50.851034
3469.911916	321797.795717	50.856039
3469.266758	321620.760204	50.861044
3468.565135	321457.508123	50.866049
3467.746690	321289.309144	50.871053
3467.640301	321117.610831	50.876058
3466.725887	320960.094959	50.881063
3465.765591	320773.890356	50.886068
3465.366479	320624.516663	50.891073
3464.332337	320443.186312	50.896077
3464.160618	320270.376386	50.901082
3463.080651	320120.091027	50.906087
3462.209072	319942.426002	50.911092
3461.843437	319774.458170	50.916097
3461.013157	319601.598337	50.921101
3460.586063	319432.952120	50.926106
3459.613984	319276.639204	50.931111
3459.027584	319103.841738	50.936116
3458.374597	318940.653860	50.941121
3457.756170	318779.879182	50.946125
3457.592573	318605.486198	50.951130
3456.592581	318444.287490	50.956135
3456.149320	318270.574677	50.961140
3455.426789	318098.204306	50.966145
3454.383076	317928.990871	50.971149
3454.254336	317757.824609	50.976154
3453.116811	317594.787433	50.981159
3452.543867	317416.764895	50.986164
3451.730226	317257.826406	50.991169
3451.265175	317093.867252	50.996173
3450.494955	316919.516216	51.001178
3449.499846	316760.452839	51.006183
3449.115344	316585.887450	51.011188
3448.523780	316422.889326	51.016193
3447.818680	316251.251386	51.021197
3447.328651	316084.875511	51.026202
3446.590994	315922.918207	51.031207
3445.763166	315739.585670	51.036212
3444.948224	315585.839254	51.041217
3444.378584	315421.130001	51.046221
3443.818153	315250.027690	51.051226
3443.183874	315095.768169	51.056231
3442.405369	314923.350230	51.061236
3441.917161	314743.552582	51.066241
3441.240167	314584.155403	51.071245
3440.319406	314425.866002	51.076250
3439.581894	314261.868974	51.081255
3439.216374	314092.592799	51.086260
3438.285674	313929.873529	51.091265
3437.572515	313769.284041	51.096269
3437.369145	313592.902483	51.101274
3436.296216	313432.318449	51.106279
3435.757971	313260.394556	51.111284
3434.887694	313104.361508	51.116289
3434.532344	312935.438400	51.121293
3433.761848	312764.823652	51.126298
3432.906044	312597.583393	51.131303
3432.114373	312428.855818	51.136308
3431.617081	312286.182249	51.141313
3431.112348	312120.795574	51.146317
3430.523977	311948.699311	51.151322
3429.473234	311785.435620	51.156327
3428.971158	311621.702972	51.161332
3428.263496	311458.537347	51.166337
3427.678857	311298.433231	51.171341
3426.988065	311124.824048	51.176346
3426.349446	310968.471284	51.181351
3425.650869	310801.636401	51.186356
3425.041996	310632.953645	51.191361
3424.119778	310471.399353	51.196365
3423.722425	310302.606280	51.201370
3422.818695	310145.785041	51.206375
3422.422510	309981.524036	51.211380
3421.472580	309819.820446	51.216385
3420.879021	309657.550991	51.221389
3420.489155	309498.203025	51.226394
3419.821647	309334.697051	51.231399
3419.447002	309160.474761	51.236404
3418.400128	308997.792268	51.241409
3417.433657	308843.576673	51.246413
3416.933578	308671.869087	51.251418
3416.159080	308506.239865	51.256423
3415.667662	308341.558797	51.261428
3414.692855	308174.203719	51.266433
3414.006965	308029.161108	51.271437
3413.845858	307858.060895	51.276442
3412.637312	307692.448303	51.281447
3412.246177	307529.405554	51.286452
3411.699872	307378.686849	51.291457
3410.710661	307219.990976	51.296461
3410.212065	307045.454299	51.301466
3409.203677	306884.367308	51.306471
3408.936531	306736.124782	51.311476
3408.061533	306578.734266	51.316481
3407.310831	306423.081023	51.321485
3406.927991	306260.086305	51.326490
3405.978767	306103.165341	51.331495
3405.346858	305939.343790	51.336500
3405.043069	305778.042174	51.341505
3403.957030	305623.918033	51.346509
3403.592601	305462.625632	51.351514
3402.584321	305292.649207	51.356519
3402.063857	305128.019622	51.361524
3401.655471	304984.253996	51.366529
3400.892142	304818.847547	51.371533
3400.128050	304662.786957	51.376538
3399.306415	304510.224108	51.381543
3398.982823	304340.571169	51.386548
3398.215351	304187.133569	51.391553
3397.216898	304028.766485	51.396557
3396.675853	303867.041792	51.401562
3396.113163	303724.903643	51.406567
3395.693745	303558.244448	51.411572
3394.816856	303396.317682	51.416577
3394.064665	303240.533793	51.421581
3393.499021	303075.832592	51.426586
3392.832675	302929.686432	51.431591
3392.536580	302760.562094	51.436596
3392.091895	302591.308267	51.441601
3390.834755	302432.954911	51.446605
3390.073394	302269.709883	51.451610
3389.462623	302114.895647	51.456615
3388.460672	301948.097589	51.461620
3387.770082	301797.828647	51.466625
3387.239543	301637.245873	51.471629
3387.130689	301482.071506	51.476634
3385.962350	301327.675724	51.481639
3385.457155	301167.088464	51.486644
3385.111325	300998.479397	51.491649
3384.221467	300855.066064	51.496653
3383.869461	300680.091039	51.501658
3383.173592	300530.942261	51.506663
3382.713963	300361.739334	51.511668
3382.083579	300211.535786	51.516673
3381.188633	300043.776566	51.521677
3380.962113	299864.298722	51.526682
3379.661181	299706.407994	51.531687
3379.028512	299533.895472	51.536692
3378.289494	299374.667711	51.541697
3377.665922	299210.404613	51.546701
3377.024721	299051.466685	51.551706
3376.195530	298898.644883	51.556711
3375.858315	298735.278321	51.561716
3374.962819	298574.088169	51.566721
3374.056189	298418.451389	51.571725
3374.011329	298252.542406	51.576730
3372.885432	298101.982454	51.581735
3372.440528	297941.993819	51.586740
3371.886168	297772.319479	51.591745
3371.082280	297608.898365	51.596749
3370.414391	297447.671221	51.601754
3369.484439	297290.305421	51.606759
3368.966141	297122.636675	51.611764
3368.421111	296966.534014	51.616769
3367.576867	296805.155943	51.621773
3366.972459	296651.583649	51.626778
3366.189400	296486.222782	51.631783
3365.375032	296336.223362	51.636788
3364.579036	296174.124062	51.641793
3364.141210	296018.563963	51.646797
3363.644616	295852.647922	51.651802
3362.553433	295712.547585	51.656807
3362.211261	295543.550813	51.661812
3361.532632	295386.092808	51.666817
3360.769768	295238.631145	51.671821
3360.533463	295077.206472	51.676826
3359.667082	294924.922188	51.681831
3358.963282	294764.106021	51.686836
3358.336134	294593.472713	51.691841
3357.532808	294442.553345	51.696845
3356.997331	294280.869777	51.701850
3356.053947	294130.176082	51.706855
3355.584116	293968.430968	51.711860
3354.774886	293818.938278	51.716865
3353.978105	293662.541860	51.721869
3353.483236	293501.004108	51.726874
3352.585966	293346.533420	51.731879
3352.244860	293194.215804	51.736884
3351.479986	293052.406761	51.741889
3350.668221	292891.071506	51.746893
3350.415196	292732.372794	51.751898
3349.590508	292574.273737	51.756903
3348.894693	292417.809583	51.761908
3348.434252	292261.384506	51.766913
3347.654966	292105.595509	51.771917
3347.148648	291938.175503	51.776922
3346.159265	291784.329601	51.781927
3345.447304	291624.684053	51.786932
3344.954098	291472.007401	51.791937
3344.343713	291316.980701	51.796941
3343.694010	291152.970051	51.801946
3342.854966	290999.711128	51.806951
3342.486049	290842.404805	51.811956
3341.499397	290692.658122	51.816961
3340.803166	290529.978767	51.821965
3340.507882	290376.226007	51.826970
3339.549134	290211.270422	51.831975
3339.061612	290053.167438	51.836980
3338.332771	289895.892032	51.841985
3337.451062	289739.404751	51.846989
3337.219084	289584.724708	51.851994
3336.540800	289436.405717	51.856999
3335.764716	289268.339098	51.862004
3334.965276	289114.283383	51.867009
3333.958551	288957.306105	51.872013
3333.826847	288801.030792	51.877018
3332.941581	288657.532112	51.882023
3332.162584	288499.576274	51.887028
3331.504140	288336.966134	51.892033
3330.929115	288194.513296	51.897037
3330.311477	288027.949023	51.902042
3329.763621	287875.788474	51.907047
3328.930138	287716.771221	51.912052
3328.788774	287563.196438	51.917057
3327.512298	287409.979394	51.922061
3326.943180	287239.739673	51.927066
3325.983063	287097.780235	51.932071
3325.544779	286938.751055	51.937076
3325.051518	286775.604684	51.942081
3324.448039	286624.114556	51.947085
3323.887443	286463.627370	51.952090
3322.881177	286321.191038	51.957095
3322.374376	286160.338663	51.962100
3321.620909	286004.058550	51.967105
3320.409274	285853.963176	51.972109
3320.258557	285698.861012	51.977114
3319.147817	285553.766779	51.982119
3318.802624	285393.346960	51.987124
3318.320667	285242.677527	51.992129
3317.322163	285088.549673	51.997133
3317.133059	284940.049539	52.002138
3316.210446	284794.212185	52.007143
3315.806253	284627.612657	52.012148
3315.293169	284473.815302	52.017153
3314.270392	284320.658812	52.022157
3313.960790	284159.163253	52.027162
3313.108261	284010.309323	52.032167
3312.401200	283855.498253	52.037172
3311.704131	283703.792674	52.042177
3310.651373	283547.686374	52.047181
3310.546501	283398.612134	52.052186
3309.209416	283249.478068	52.057191
3308.751209	283078.607899	52.062196
3308.301007	282932.084035	52.067201
3307.582933	282777.656414	52.072205
3306.910546	282620.037994	52.077210
3305.996923	282478.935644	52.082215
3306.001647	282318.510411	52.087220
3305.094322	282165.360508	52.092225
3304.250815	282017.396000	52.097229
3303.792430	281858.775741	52.102234
3302.714475	281712.656494	52.107239
3302.027691	281554.887273	52.112244
3301.695353	281397.087422	52.117249
3300.682002	281258.751156	52.122253
3300.685319	281102.349840	52.127258
3299.665535	280951.764283	52.132263
3298.896590	280792.123239	52.137268
3298.051063	280644.770003	52.142273
3297.279758	280498.780290	52.147277
3296.781193	280346.380330	52.152282
3296.447487	280197.596237	52.157287
3295.706259	280047.552227	52.162292
3294.965733	279893.305805	52.167297
3294.212631	279746.803724	52.172301
3293.670581	279586.744547	52.177306
3293.077238	279434.614114	52.182311
3292.828102	279282.836709	52.187316
3292.138346	279126.519206	52.192321
3291.035857	278970.572587	52.197325
3290.862254	278795.530559	52.202330
3289.916338	278653.872355	52.207335
3289.169137	278490.305375	52.212340
3288.528837	278338.309576	52.217345
3287.729002	278189.115050	52.222349
3287.137268	278030.820850	52.227354
3286.445116	277881.329111	52.232359
3285.873031	277726.597349	52.237364
3285.368257	277570.479635	52.242369
3284.387294	277418.486706	52.247373
3283.930243	277265.519501	52.252378
3282.826053	277111.635916	52.257383
3282.309979	276948.770827	52.262388
3281.830345	276801.741302	52.267393
3281.133164	276658.031606	52.272397
3280.338652	276499.591102	52.277402
3279.354098	276351.215201	52.282407
3278.950176	276199.512964	52.287412
3278.375384	276049.569604	52.292417
3277.606605	275904.979821	52.297421
3277.130526	275750.079973	52.302426
3276.396603	275606.758094	52.307431
3275.570928	275449.061087	52.312436
3274.973490	275293.849348	52.317441
3274.360558	275145.771212	52.322445
3273.854570	275000.375811	52.327450
3272.871398	274849.987687	52.332455
3272.369267	274688.699408	52.337460
3271.539153	274545.316358	52.342465
3270.933410	274405.234180	52.347469
3270.549022	274249.759555	52.352474
3269.622485	274100.355770	52.357479
3268.882125	273954.284369	52.362484
3268.302412	273807.474450	52.367489
3267.608362	273650.342465	52.372493
3267.552343	273502.787547	52.377498
3266.352281	273355.464551	52.382503
3265.839918	273192.751756	52.387508
3265.069934	273041.311281	52.392513
3264.142912	272903.393900	52.397517
3263.966965	272747.708141	52.402522
3263.022094	272597.874416	52.407527
3262.298224	272443.854404	52.412532
3261.789387	272286.514977	52.417537
3260.893708	272138.863804	52.422541
3260.313199	271987.036919	52.427546
3259.325088	271841.157722	52.432551
3258.732860	271698.297590	52.437556
3258.511783	271544.376441	52.442561
3257.329859	271415.591753	52.447565
3256.711961	271255.697427	52.452570
3256.180431	271115.807572	52.457575
3255.534595	270973.108838	52.462580
3254.864841	270821.398124	52.467585
3254.037412	270681.045782	52.472589
3253.790506	270529.191825	52.477594
3253.116567	270390.750844	52.482599
3252.458490	270243.368004	52.487604
3251.906728	270084.507639	52.492609
3251.201553	269943.754066	52.497613
3250.497372	269782.014494	52.502618
3249.866415	269641.962353	52.507623
3249.694985	269489.536367	52.512628
3248.816248	269333.325663	52.517633
3247.813646	269177.491148	52.522637
3247.282553	269028.203827	52.527642
3246.276525	268884.492818	52.532647
3245.569164	268727.618449	52.537652
3244.893344	268573.871725	52.542657
3243.996652	268437.376508	52.547661
3243.613905	268283.965522	52.552666
3242.602287	268149.398674	52.557671
3242.168210	268002.744965	52.562676
3241.565070	267855.812423	52.567681
3240.807803	267716.773978	52.572685
3240.515005	267569.766953	52.577690
3239.274481	267428.843986	52.582695
3239.066969	267279.582354	52.587700
3238.412857	267131.970445	52.592705
3237.557131	266990.044408	52.597709
3237.031135	266850.078235	52.602714
3236.248314	266702.665100	52.607719
3235.921736	266556.580581	52.612724
3235.210814	266410.225827	52.617729
3234.331432	266268.354694	52.622733
3234.095892	266128.266391	52.627738
3233.176060	265988.617475	52.632743
3232.604278	265824.413234	52.637748
3232.172224	265670.985422	52.642753
3231.006951	265524.269894	52.647757
3230.532479	265374.159754	52.652762
3229.643815	265238.861202	52.657767
3229.215916	265086.069657	52.662772
3228.432882	264936.543329	52.667777
3227.473730	264799.345979	52.672781
3227.125250	264650.667864	52.677786
3226.440107	264507.442288	52.682791
3225.782693	264362.429622	52.687796
3225.083221	264209.503122	52.692801
3224.374937	264057.367589	52.697805
3223.696464	263917.884985	52.702810
3222.959878	263777.851337	52.707815
3222.395788	263637.892327	52.712820
3221.731495	263488.882641	52.717825
3221.134149	263350.304280	52.722829
3220.952013	263193.450729	52.727834
3219.715252	263054.668037	52.732839
3219.027970	262902.809848	52.737844
3218.717703	262761.002833	52.742849
3218.049406	262607.409965	52.747853
3217.285426	262456.149886	52.752858
3216.564518	262318.813976	52.757863
3215.943295	262164.297038	52.762868
3215.226235	262024.286530	52.767873
3214.670084	261872.357164	52.772877
3213.884389	261721.355565	52.777882
3212.987223	261591.586340	52.782887
3212.210011	261427.747789	52.787892
3211.984750	261291.021569	52.792897
3211.073936	261144.878940	52.797901
3210.402810	261001.296174	52.802906
3209.810123	260858.261362	52.807911
3209.232584	260713.645229	52.812916
3208.533425	260561.026093	52.817921
3207.696449	260422.436068	52.822925
3207.094874	260269.012160	52.827930
3206.114278	260129.375368	52.832935
3205.595933	259988.723214	52.837940
3205.076778	259848.045796	52.842945
3204.202660	259700.421023	52.847949
3204.067165	259562.178887	52.852954
3203.129980	259422.153595	52.857959
3202.617314	259271.033762	52.862964
3201.667456	259128.234676	52.867969
3200.853155	258999.344966	52.872973
3200.363802	258846.846456	52.877978
3199.697542	258715.463125	52.882983
3199.119180	258575.941829	52.887988
3198.371491	258430.971897	52.892993
3197.848284	258288.946230	52.897997
3197.091058	258138.960897	52.903002
3196.564893	258005.824007	52.908007
3195.658005	257852.653642	52.913012
3195.041620	257707.943526	52.918017
3194.177020	257582.449712	52.923021
3193.867410	257427.198678	52.928026
3193.074921	257289.214610	52.933031
3192.370239	257143.856676	52.938036
3191.830218	257009.754807	52.943041
3191.210072	256872.660555	52.948045
3190.650032	256723.663658	52.953050
3190.008063	256578.805524	52.958055
3189.265841	256437.579699	52.963060
3188.467498	256289.664965	52.968065
3187.283986	256159.281786	52.973069
3187.402184	256009.261259	52.978074
3186.576708	255873.575367	52.983079
3185.560127	255729.031761	52.988084
3185.184142	255590.830090	52.993089
3184.321948	255448.605232	52.998093
3183.746807	255309.976854	53.003098
3182.917484	255171.363322	53.008103
3182.215328	255028.553165	53.013108
3181.888914	254883.111488	53.018113
3180.720707	254752.879595	53.023117
3180.515255	254605.101484	53.028122
3179.532391	254479.908385	53.033127
3178.747226	254336.627995	53.038132
3178.417892	254194.370668	53.043137
3177.751727	254069.942671	53.048141
3177.171631	253919.397535	53.053146
3176.288531	253788.204378	53.058151
3175.851730	253651.108781	53.063156
3175.288246	253504.304983	53.068161
3174.429289	253366.079449	53.073165
3173.994182	253220.146906	53.078170
3172.913675	253082.160376	53.083175
3172.716572	252946.886456	53.088180
3171.999308	252806.958120	53.093185
3171.127721	252664.660436	53.098189
3170.617122	252519.428008	53.103194
3169.843592	252383.736386	53.108199
3169.316357	252241.104424	53.113204
3168.854066	252104.981771	53.118209
3167.712591	251962.701894	53.123213
3167.311421	251819.413666	53.128218
3166.446138	251680.808449	53.133223
3165.688676	251537.143900	53.138228
3165.379218	251398.756566	53.143233
3164.595288	251265.053865	53.148237
3163.998808	251112.425449	53.153242
3163.371513	250978.850992	53.158247
3162.302373	250835.720225	53.163252
3161.902678	250694.622840	53.168257
3161.117836	250559.825795	53.173261
3160.585957	250418.011038	53.178266
3159.822895	250281.631860	53.183271
3159.029847	250136.675375	53.188276
3158.717204	250002.517138	53.193281
3157.696365	249874.200996	53.198285
3157.181193	249725.941227	53.203290
3156.146753	249593.756587	53.208295
3155.558394	249455.898897	53.213300
3155.345812	249325.290680	53.218305
3154.514488	249189.381639	53.223309
3154.004792	249047.921128	53.228314
3153.093485	248900.055887	53.233319
3152.666797	248762.224167	53.238324
3152.040678	248620.680609	53.243329
3151.242279	248488.306773	53.248333
3151.109487	248344.851853	53.253338
3149.841400	248204.352513	53.258343
3148.936717	248060.943608	53.263348
3148.411740	247919.435641	53.268353
3147.747143	247790.377301	53.273357
3147.011631	247655.091137	53.278362
3146.285485	247522.579403	53.283367
3145.905662	247389.147148	53.288372
3145.320475	247256.613353	53.293377
3144.466811	247113.833953	53.298381
3144.038751	246966.199772	53.303386
3143.129107	246835.398453	53.308391
3142.296730	246696.817963	53.313396
3141.921677	246569.370179	53.318401
3141.163187	246430.014287	53.323405
3140.683269	246291.887738	53.328410
3140.069470	246157.525969	53.333415
3139.395062	246018.284513	53.338420
3138.860236	245876.067095	53.343425
3138.034688	245737.231824	53.348429
3137.669741	245595.751785	53.353434
3136.251273	245455.966536	53.358439
3135.467975	245322.854755	53.363444
3135.274096	245189.726231	53.368449
3134.536883	245062.158897	53.373453
3133.813441	244919.386626	53.378458
3133.114385	244792.424683	53.383463
3132.554996	244650.416170	53.388468
3131.794779	244512.514050	53.393473
3130.835595	244385.950178	53.398477
3130.724429	244245.577354	53.403482
3130.113544	244111.904737	53.408487
3129.187703	243981.312465	53.413492
3128.832587	243837.540873	53.418497
3127.832144	243708.845112	53.423501
3127.313928	243571.058491	53.428506
3126.722845	243438.809492	53.433511
3126.022808	243292.673905	53.438516
3125.472145	243159.476592	53.443521
3124.334262	243021.788628	53.448525
3123.565308	242885.901385	53.453530
3122.962575	242756.889009	53.458535
3122.160038	242624.801655	53.463540
3121.684846	242495.336464	53.468545
3121.069866	242372.336162	53.473549
3120.627706	242227.994494	53.478554
3119.772556	242096.527192	53.483559
3119.637134	241967.187046	53.488564
3118.932090	241833.098859	53.493569
3117.833825	241702.663585	53.498573
3117.337741	241557.159868	53.503578
3116.737499	241425.678423	53.508583
3116.065868	241303.783157	53.513588
3115.116131	241154.302829	53.518593
3114.570951	241023.551591	53.523597
3114.069569	240886.096368	53.528602
3113.306813	240748.453487	53.533607
3112.842625	240616.187474	53.538612
3112.238938	240488.705558	53.543617
3111.417351	240355.452353	53.548621
3110.754761	240208.601568	53.553626
3109.657359	240076.971131	53.558631
3108.951672	239945.202464	53.563636
3108.720052	239817.229515	53.568641
3107.984822	239684.396319	53.573645
3107.742264	239539.720786	53.578650
3106.662614	239409.488851	53.583655
3105.825846	239281.714130	53.588660
3105.346346	239137.534967	53.593665
3104.792198	239017.304169	53.598669
3103.818839	238877.379629	53.603674
3103.283401	238745.763672	53.608679
3102.589145	238604.267458	53.613684
3101.946010	238476.361163	53.618689
3101.476176	238350.210076	53.623693
3100.858337	238210.357442	53.628698
3100.056033	238085.048661	53.633703
3099.351262	237942.561871	53.638708
3098.769722	237804.231853	53.643713
3097.886126	237667.757751	53.648717
3097.658152	237544.344892	53.653722
3096.910216	237410.777994	53.658727
3096.324721	237278.458747	53.663732
3095.505239	237129.625237	53.668737
3094.686645	237009.591293	53.673741
3094.091627	236868.489072	53.678746
3093.395782	236734.507363	53.683751
3092.482282	236609.498014	53.688756
3091.884303	236467.250936	53.693761
3091.283129	236339.264166	53.698765
3090.642481	236208.941154	53.703770
3090.137074	236075.235718	53.708775
3089.319873	235944.355320	53.713780
3088.506299	235818.032473	53.718785
3088.015850	235677.373663	53.723789
3087.663525	235540.258061	53.728794
3086.801657	235419.952711	53.733799
3085.904554	235290.893694	53.738804
3085.429236	235160.596779	53.743809
3084.518459	235025.276296	53.748813
3084.021014	234890.221603	53.753818
3083.140197	234778.577515	53.758823
3082.569864	234635.946668	53.763828
3082.105468	234507.329442	53.768833
3081.069239	234380.076038	53.773837
3081.108017	234242.391050	53.778842
3079.998912	234119.478235	53.783847
3079.477824	233994.537326	53.788852
3078.760694	233848.366029	53.793857
3077.777124	233727.369024	53.798861
3077.313374	233599.058440	53.803866
3076.409614	233471.403309	53.808871
3075.946942	233347.116019	53.813876
3075.381439	233202.245765	53.818881
3074.382163	233078.094674	53.823885
3074.113442	232944.941632	53.828890
3073.403581	232822.960324	53.833895
3072.417501	232698.298384	53.838900
3071.974882	232566.879390	53.843905
3071.180258	232439.641227	53.848909
3070.837298	232317.296951	53.853914
3070.101085	232179.406548	53.858919
3069.359816	232049.181355	53.863924
3068.897357	231926.500025	53.868929
3067.915719	231802.067732	53.873933
3067.345192	231659.848725	53.878938
3066.899811	231538.922107	53.883943
3065.839285	231411.014484	53.888948
3065.498150	231274.005000	53.893953
3064.790049	231156.965265	53.898957
3064.141352	231023.365848	53.903962
3063.372532	230899.792267	53.908967
3062.713790	230770.752536	53.913972
3062.147936	230638.439140	53.918977
3061.422164	230516.819847	53.923981
3060.798233	230378.990755	53.928986
3060.145412	230249.161508	53.933991
3059.295636	230119.618241	53.938996
3058.693315	229991.741943	53.944001
3057.850494	229869.250886	53.949005
3057.252614	229731.520514	53.954010
3056.491575	229606.266998	53.959015
3056.051082	229475.488646	53.964020
3055.787542	229353.390390	53.969025
3054.592047	229231.796270	53.974029
3054.275182	229091.960020	53.979034
3053.689645	228972.586730	53.984039
3052.665763	228838.286111	53.989044
3052.228417	228714.688559	53.994049
3051.510431	228578.226619	53.999053
3050.873072	228448.270266	54.004058
3049.966556	228327.599207	54.009063
3049.394316	228200.662830	54.014068
3048.891362	228073.562906	54.019073
3047.954165	227955.468823	54.024077
3047.162497	227824.621228	54.029082
3046.528287	227702.482119	54.034087
3045.889632	227573.902203	54.039092
3045.586370	227442.366825	54.044097
3044.927964	227328.659728	54.049101
3043.860489	227196.507317	54.054106
3043.240126	227078.517073	54.059111
3042.510497	226945.344063	54.064116
3042.179548	226815.609047	54.069121
3041.177491	226703.612152	54.074125
3040.747353	226562.257580	54.079130
3040.128905	226453.943057	54.084135
3039.336082	226326.178742	54.089140
3038.818271	226195.926860	54.094145
3037.837253	226074.685222	54.099149
3037.423915	225949.942175	54.104154
3036.613595	225826.751602	54.109159
3036.305491	225695.690769	54.114164
3036.006902	225574.061790	54.119169
3034.564590	225452.079349	54.124173
3034.271460	225320.303855	54.129178
3033.559657	225192.210229	54.134183
3032.798331	225066.365164	54.139188
3032.441775	224939.705145	54.144193
3031.535718	224817.918847	54.149197
3031.262817	224690.647661	54.154202
3030.311947	224561.472627	54.159207
3029.749881	224439.976171	54.164212
3028.979320	224298.666681	54.169217
3028.168122	224174.383984	54.174221
3027.637974	224041.566049	54.179226
3026.785993	223909.435781	54.184231
3025.983045	223779.576644	54.189236
3025.454358	223654.600817	54.194241
3024.549670	223532.701708	54.199245
3024.030200	223405.064256	54.204250
3023.274356	223278.533741	54.209255
3022.871645	223158.477979	54.214260
3022.427098	223032.789684	54.219265
3021.154762	222917.671113	54.224269
3020.862028	222791.628202	54.229274
3019.906918	222662.724292	54.234279
3019.337193	222547.889684	54.239284
3018.978731	222426.695102	54.244289
3017.752823	222298.382049	54.249293
3017.517200	222178.059500	54.254298
3016.787830	222054.772889	54.259303
3016.129179	221938.540273	54.264308
3015.596784	221811.722208	54.269313
3014.857041	221689.112507	54.274317
3014.206053	221560.658778	54.279322
3013.633509	221448.881389	54.284327
3012.493795	221318.048617	54.289332
3012.267312	221195.816740	54.294337
3011.277755	221072.776592	54.299341
3010.705459	220944.960669	54.304346
3010.012846	220835.061714	54.309351
3009.386623	220715.554369	54.314356
3008.878979	220584.533725	54.319361
3007.973992	220470.175422	54.324365
3007.436150	220350.412816	54.329370
3006.795968	220226.351331	54.334375
3005.940995	220109.643458	54.339380
3005.543424	219991.934123	54.344385
3005.030199	219871.277344	54.349389
3004.552438	219745.828920	54.354394
3003.485029	219631.675845	54.359399
3002.940830	219506.518395	54.364404
3002.712576	219371.318672	54.369409
3001.804829	219248.663234	54.374413
3001.257423	219122.730469	54.379418
3000.654914	218998.105026	54.384423
2999.673494	218866.016833	54.389428
2998.775643	218744.086251	54.394433
2997.915291	218614.283334	54.399437
2997.780613	218495.414652	54.404442
2996.954040	218383.453028	54.409447
2996.060486	218266.334179	54.414452
2995.621083	218138.031171	54.419457
2994.974459	218016.927640	54.424461
2994.529596	217902.551481	54.429466
2993.475014	217781.640221	54.434471
2992.936291	217651.393555	54.439476
2992.102009	217528.576700	54.444481
2991.550653	217418.736958	54.449485
2990.971768	217287.249890	54.454490
2990.426247	217168.575764	54.459495
2989.602057	217050.569666	54.464500
2988.962184	216909.877275	54.469505
2988.234578	216803.630474	54.474509
2987.745264	216682.618907	54.479514
2986.870595	216563.336022	54.484519
2986.370795	216431.876240	54.489524
2985.589139	216319.096169	54.494529
2984.809621	216204.966702	54.499533
2984.559980	216075.262748	54.504538
2983.671422	215953.220999	54.509543
2982.968980	215832.104653	54.514548
2982.533375	215707.535015	54.519553
2981.958630	215595.563470	54.524557
2981.443625	215464.591640	54.529562
2980.415070	215330.761068	54.534567
2979.819203	215212.543790	54.539572
2978.998146	215089.270972	54.544577
2978.234389	214978.297736	54.549581
2977.659085	214847.132995	54.554586
2976.979682	214729.426199	54.559591
2976.242351	214607.286570	54.564596
2975.823394	214485.758640	54.569601
2975.236335	214373.676523	54.574605
2974.067978	214252.280381	54.579610
2973.753645	214129.056399	54.584615
2973.000345	214012.953607	54.589620
2972.162693	213886.669035	54.594625
2971.509347	213774.063839	54.599629
2971.214811	213649.081121	54.604634
2970.326263	213529.054845	54.609639
2969.443868	213412.884449	54.614644
2969.093878	213283.494531	54.619649
2968.513194	213177.484762	54.624653
2968.110634	213045.583469	54.629658
2966.846083	212931.421827	54.634663
2966.573239	212810.599357	54.639668
2966.049477	212687.983998	54.644673
2965.120297	212567.482260	54.649677
2964.871854	212445.447447	54.654682
2963.825252	212315.966088	54.659687
2963.054096	212194.396339	54.664692
2962.477312	212073.114246	54.669697
2961.729719	211955.995986	54.674701
2961.296342	211830.058702	54.679706
2960.398106	211714.784815	54.684711
2959.786561	211587.234325	54.689716
2959.361684	211471.007723	54.694721
2958.272039	211357.266665	54.699725
2957.591331	211230.415140	54.704730
2957.140785	211116.089684	54.709735
2956.078700	210995.115574	54.714740
2955.762871	210869.848880	54.719745
2955.055095	210762.081353	54.724749
2954.419364	210636.725764	54.729754
2953.504395	210520.540316	54.734759
2952.654688	210413.979524	54.739764
2952.275322	210293.433241	54.744769
2951.455220	210185.302665	54.749773
2951.047176	210064.315901	54.754778
2950.542702	209947.073790	54.759783
2949.623612	209839.684952	54.764788
2948.987743	209715.209432	54.769793
2948.436231	209604.657317	54.774797
2948.067348	209477.658163	54.779802
2947.207849	209367.804327	54.784807
2946.607174	209242.076909	54.789812
2946.041633	209115.796912	54.794817
2945.228510	209005.936382	54.799821
2944.610844	208877.119673	54.804826
2944.241572	208758.254786	54.809831
2943.123205	208646.215964	54.814836
2942.772620	208517.230460	54.819841
2941.909662	208400.760777	54.824845
2941.431221	208261.067067	54.829850
2940.499138	208158.417729	54.834855
2939.861068	208040.487701	54.839860
2939.322038	207917.985938	54.844865
2938.446685	207805.910200	54.849869
2937.792158	207675.307371	54.854874
2937.638287	207561.208814	54.859879
2936.349181	207432.043314	54.864884
2935.995254	207316.933286	54.869889
2935.142096	207201.991607	54.874893
2935.021613	207081.207056	54.879898
2933.948793	206965.498818	54.884903
2933.241386	206837.298843	54.889908
2932.853364	206716.175587	54.894913
2931.775896	206594.996286	54.899917
2931.045237	206480.100246	54.904922
2930.512740	206370.963716	54.909927
2930.033776	206253.457472	54.914932
2929.411770	206138.863064	54.919937
2928.594554	206021.576283	54.924941
2928.141827	205886.274766	54.929946
2927.316143	205779.323829	54.934951
2926.582196	205658.792037	54.939956
2926.297850	205537.374814	54.944961
2925.267078	205425.162755	54.949965
2924.387016	205301.562294	54.954970
2923.656975	205184.543381	54.959975
2923.267099	205070.041588	54.964980
2922.719034	204958.212163	54.969985
2921.817152	204842.621055	54.974989
2921.179328	204721.961458	54.979994
2920.681394	204608.177641	54.984999
2919.816524	204496.093840	54.990004
2919.317379	204375.374836	54.995009
2918.282440	204260.785892	55.000013
2917.940075	204142.040582	55.005018
2917.407547	204031.788556	55.010023
2916.578113	203914.953410	55.015028
2915.942378	203803.712799	55.020033
2915.385215	203682.520855	55.025037
2914.931323	203559.098476	55.030042
2914.262713	203444.389549	55.035047
2913.405946	203325.740117	55.040052
2913.043851	203204.938272	55.045057
2912.184762	203102.986225	55.050061
2911.650688	202978.814252	55.055066
2911.057244	202856.828091	55.060071
2910.386379	202731.774781	55.065076
2909.821782	202598.064047	55.070081
2908.810288	202492.586721	55.075085
2908.489190	202359.219782	55.080090
2907.525415	202242.269400	55.085095
2907.063588	202125.901531	55.090100
2906.380739	202001.488048	55.095105
2905.534222	201871.781407	55.100109
2905.156319	201754.281167	55.105114
2904.024212	201643.530667	55.110119
2903.404711	201517.199395	55.115124
2902.963211	201403.285879	55.120129
2902.078634	201286.770379	55.125133
2901.351019	201164.401970	55.130138
2900.820335	201047.080139	55.135143
2900.166141	200935.097378	55.140148
2899.194472	200810.146950	55.145153
2898.545677	200701.281556	55.150157
2897.842232	200590.592571	55.155162
2896.988617	200471.732434	55.160167
2896.604345	200365.180028	55.165172
2896.293008	200248.423282	55.170177
2895.340871	200136.552970	55.175181
2895.126023	200012.146266	55.180186
2894.151189	199898.320348	55.185191
2893.355013	199782.112214	55.190196
2892.672636	199674.653981	55.195201
2892.088100	199553.106420	55.200205
2891.574209	199432.973167	55.205210
2890.668550	199320.944493	55.210215
2890.105215	199208.034720	55.215220
2889.443897	199088.129187	55.220225
2888.524454	198985.100028	55.225229
2888.090098	198870.478117	55.230234
2887.435912	198756.082137	55.235239
2886.618645	198638.047437	55.240244
2886.181390	198525.322752	55.245249
2885.346513	198418.311125	55.250253
2884.956104	198299.178875	55.255258
2883.951874	198184.254215	55.260263
2883.165572	198079.513335	55.265268
2882.859882	197956.767320	55.270273
2882.173120	197846.641279	55.275277
2881.383346	197733.388769	55.280282
2880.824833	197620.761570	55.285287
2880.144285	197497.477927	55.290292
2879.855518	197389.847490	55.295297
2878.852954	197278.729230	55.300301
2878.283240	197158.648170	55.305306
2877.498326	197039.950269	55.310311
2877.131921	196930.246247	55.315316
2876.316288	196804.198962	55.320321
2875.255853	196699.326122	55.325325
2874.602362	196585.863668	55.330330
2874.356096	196485.939403	55.335335
2873.316485	196362.702591	55.340340
2872.885100	196251.190713	55.345345
2871.951782	196142.417945	55.350349
2871.497692	196022.066735	55.355354
2870.725465	195907.403047	55.360359
2870.079016	195799.603527	55.365364
2869.796578	195688.692777	55.370369
2868.585712	195576.796828	55.375373
2868.199033	195463.383681	55.380378
2867.655093	195350.708242	55.385383
2866.789729	195239.941673	55.390388
2866.019951	195117.225006	55.395393
2865.089248	195017.730096	55.400397
2864.176316	194903.854398	55.405402
2863.785937	194797.950513	55.410407
2863.021045	194701.076568	55.415412
2862.969633	194581.721100	55.420417
2861.995240	194475.757684	55.425421
2861.532494	194361.061215	55.430426
2860.851539	194251.094673	55.435431
2860.309701	194150.954605	55.440436
2859.539716	194037.389057	55.445441
2858.713023	193932.039596	55.450445
2858.287444	193812.439839	55.455450
2857.514089	193702.120149	55.460455
2856.852621	193593.996913	55.465460
2856.431148	193480.720988	55.470465
2855.659469	193371.012505	55.475469
2855.021469	193254.921286	55.480474
2854.106033	193150.592703	55.485479
2853.555019	193041.842449	55.490484
2853.267996	192921.650339	55.495489
2852.351313	192804.191998	55.500493
2851.745262	192682.333319	55.505498
2851.272062	192569.754743	55.510503
2850.393436	192468.602640	55.515508
2849.728399	192342.758991	55.520513
2848.878562	192236.856985	55.525517
2848.240734	192136.227266	55.530522
2847.736671	192017.165950	55.535527
2847.091060	191900.137616	55.540532
2846.735735	191781.943950	55.545537
2845.853280	191679.750785	55.550541
2844.936908	191568.796931	55.555546
2844.587636	191453.974749	55.560551
2843.485361	191347.732962	55.565556
2843.124248	191227.047833	55.570561
2842.421000	191117.804328	55.575565
2841.507790	190998.339553	55.580570
2841.139601	190887.758485	55.585575
2840.523523	190782.433347	55.590580
2839.887050	190665.406557	55.595585
2839.167733	190554.220268	55.600589
2838.642577	190442.112887	55.605594
2838.094623	190324.449491	55.610599
2837.516312	190210.175464	55.615604
2836.741387	190087.395851	55.620609
2835.838075	189974.929602	55.625613
2835.088251	189863.635249	55.630618
2834.314754	189751.874166	55.635623
2833.671425	189642.777217	55.640628
2833.090485	189528.759699	55.645633
2832.226624	189416.084966	55.650637
2831.589680	189304.850386	55.655642
2831.054536	189199.783110	55.660647
2830.209801	189098.251068	55.665652
2829.815318	188986.838895	55.670657
2828.967883	188873.119615	55.675661
2828.576954	188760.715062	55.680666
2827.722589	188651.870110	55.685671
2826.996559	188541.567459	55.690676
2826.515499	188437.918229	55.695681
2825.518769	188328.638571	55.700685
2825.091329	188223.327425	55.705690
2824.121894	188107.797319	55.710695
2823.620131	188008.592391	55.715700
2822.911219	187884.294131	55.720705
2822.363220	187785.605890	55.725709
2821.290888	187675.016637	55.730714
2820.963429	187591.166069	55.735719
2820.103053	187471.460145	55.740724
2819.747176	187363.633366	55.745729
2818.799200	187260.760422	55.750733
2818.461473	187153.007593	55.755738
2817.860663	187039.762624	55.760743
2817.075452	186932.132068	55.765748
2816.616987	186814.984920	55.770753
2815.615986	186715.429290	55.775757
2815.051827	186602.434034	55.780762
2814.278411	186501.392538	55.785767
2813.762790	186392.550149	55.790772
2813.415738	186275.768391	55.795777
2812.315510	186176.865739	55.800781
2811.873391	186066.931140	55.805786
2811.371995	185956.599100	55.810791
2810.376268	185859.766943	55.815796
2809.690218	185748.561417	55.820801
2809.283054	185635.798129	55.825805
2808.625328	185518.647707	55.830810
2807.903521	185419.661335	55.835815
2807.181853	185305.434820	55.840820
2806.743554	185199.140067	55.845825
2805.818000	185087.503406	55.850829
2805.363764	184983.437935	55.855834
2805.037927	184874.645466	55.860839
2803.969347	184754.839729	55.865844
2803.497504	184634.863478	55.870849
2802.559343	184531.715301	55.875853
2801.740231	184414.835021	55.880858
2801.172786	184310.051213	55.885863
2800.344618	184210.664555	55.890868
2800.041497	184102.557310	55.895873
2799.103486	183996.090133	55.900877
2798.465488	183885.466787	55.905882
2797.865829	183785.039927	55.910887
2797.039118	183667.819346	55.915892
2796.246766	183566.825611	55.920897
2795.968233	183460.318880	55.925901
2795.239806	183350.805196	55.930906
2794.600387	183251.136379	55.935911
2793.739985	183138.641992	55.940916
2793.516971	183034.468136	55.945921
2792.424148	182926.488836	55.950925
2791.825053	182817.108646	55.955930
2791.286491	182711.230066	55.960935
2790.704420	182606.757910	55.965940
2790.127100	182501.356642	55.970945
2789.213279	182392.803319	55.975949
2788.422555	182284.408860	55.980954
2787.916943	182176.859955	55.985959
2786.677142	182072.416926	55.990964
2786.627173	181954.747168	55.995969
2786.183223	181855.254102	56.000973
2785.285503	181749.282095	56.005978
2784.889901	181646.067477	56.010983
2783.999592	181545.793548	56.015988
2783.423310	181420.703560	56.020993
2782.571126	181326.568037	56.025997
2781.814333	181209.419300	56.031002
2781.337333	181104.285382	56.036007
2780.303981	181005.320112	56.041012
2780.151529	180890.735056	56.046017
2779.357921	180801.832129	56.051021
2778.793598	180691.853942	56.056026
2777.754715	180580.005021	56.061031
2776.945370	180475.510406	56.066036
2776.479125	180369.142738	56.071041
2775.859439	180266.030522	56.076045
2775.271807	180167.594435	56.081050
2774.745073	180060.817355	56.086055
2773.818161	179955.986475	56.091060
2773.484612	179849.001250	56.096065
2772.781409	179745.941681	56.101069
2771.934636	179633.695942	56.106074
2771.590741	179521.727006	56.111079
2770.659299	179425.674816	56.116084
2770.096241	179326.995111	56.121089
2769.324099	179222.574003	56.126093
2769.083440	179110.144615	56.131098
2768.276701	178993.645863	56.136103
2767.176955	178898.995253	56.141108
2766.683561	178778.707900	56.146113
2766.078944	178676.640174	56.151117
2765.574755	178579.606436	56.156122
2764.676325	178473.057594	56.161127
2763.866474	178363.823909	56.166132
2763.499369	178251.989219	56.171137
2762.426829	178152.502609	56.176141
2761.836602	178043.692873	56.181146
2761.394049	177941.601270	56.186151
2760.635947	177834.777445	56.191156
2760.050403	177731.411638	56.196161
2759.108599	177632.401616	56.201165
2758.615092	177529.873922	56.206170
2757.964481	177431.174395	56.211175
2757.293961	177328.827865	56.216180
2756.922296	177214.541893	56.221185
2755.997035	177124.319364	56.226189
2755.356835	177008.613801	56.231194
2754.770601	176903.202407	56.236199
2753.849135	176807.879650	56.241204
2753.503375	176700.700904	56.246209
2752.796716	176603.678415	56.251213
2752.288675	176498.789865	56.256218
2751.593672	176388.500251	56.261223
2750.763524	176279.466063	56.266228
2750.585569	176169.158735	56.271233
2749.434267	176075.832777	56.276237
2749.120078	175960.917965	56.281242
2748.234018	175853.966919	56.286247
2747.077433	175755.529623	56.291252
2746.965083	175652.908079	56.296257
2746.016667	175545.280916	56.301261
2745.214950	175437.058467	56.306266
2744.761215	175333.219950	56.311271
2744.152648	175242.938691	56.316276
2743.556165	175131.848325	56.321281
2742.931868	175039.738554	56.326285
2742.238492	174928.943898	56.331290
2741.733237	174819.277119	56.336295
2740.734144	174715.234048	56.341300
2740.336454	174610.409197	56.346305
2739.212293	174506.157549	56.351309
2738.701925	174405.509950	56.356314
2738.397232	174305.682142	56.361319
2737.415309	174208.848878	56.366324
2736.960211	174088.963462	56.371329
2735.719845	173996.152423	56.376333
2735.179049	173897.176990	56.381338
2734.939124	173802.541864	56.386343
2734.257474	173694.712057	56.391348
2733.756952	173596.710274	56.396353
2732.864343	173494.840997	56.401357
2732.194029	173391.766722	56.406362
2731.398833	173285.698361	56.411367
2731.184722	173179.512802	56.416372
2730.584035	173061.116086	56.421377
2729.409788	172971.527286	56.426381
2729.180481	172859.571123	56.431386
2728.647941	172759.401745	56.436391
2727.771668	172654.123697	56.441396
2726.900815	172548.781483	56.446401
2726.213748	172447.976055	56.451405
2725.725619	172340.640697	56.456410
2724.896479	172235.979461	56.461415
2723.923378	172141.591611	56.466420
2723.376843	172030.730885	56.471425
2722.706286	171944.383893	56.476429
2722.078177	171838.801650	56.481434
2721.732944	171730.974778	56.486439
2721.114407	171623.420407	56.491444
2720.191443	171516.970091	56.496449
2719.457423	171422.253606	56.501453
2718.976421	171312.300176	56.506458
2718.157137	171217.190745	56.511463
2717.449578	171120.588655	56.516468
2716.662989	171016.648821	56.521473
2716.092168	170920.725010	56.526477
2715.394403	170824.325579	56.531482
2714.891707	170724.105810	56.536487
2714.168402	170615.706061	56.541492
2713.713714	170516.623753	56.546497
2712.995007	170417.545371	56.551501
2712.350484	170316.878596	56.556506
2711.730110	170217.187457	56.561511
2710.781853	170117.866436	56.566516
2710.365549	170008.224376	56.571521
2709.762817	169913.745117	56.576525
2709.098414	169811.925584	56.581530
2708.376846	169706.580132	56.586535
2707.599311	169608.416037	56.591540
2707.117886	169496.674784	56.596545
2706.061497	169414.133242	56.601549
2705.579502	169307.021478	56.606554
2705.135349	169217.694458	56.611559
2704.368488	169115.282613	56.616564
2703.864394	169004.105916	56.621569
2703.162181	168903.909779	56.626573
2702.216668	168801.781405	56.631578
2702.013971	168693.419060	56.636583
2701.124325	168598.047492	56.641588
2700.802267	168488.382140	56.646593
2699.860006	168385.109904	56.651597
2699.476401	168279.816584	56.656602
2698.689509	168170.251221	56.661607
2698.128303	168076.164136	56.666612
2697.631749	167957.359612	56.671617
2697.088902	167856.746796	56.676621
2695.992268	167755.815063	56.681626
2695.333307	167645.239105	56.686631
2694.597904	167537.193345	56.691636
2693.738946	167431.710658	56.696641
2692.946051	167333.173404	56.701645
2692.504787	167236.411790	56.706650
2692.002792	167125.888789	56.711655
2691.188482	167035.404838	56.716660
2690.430594	166928.292648	56.721665
2689.732697	166836.697179	56.726669
2689.162752	166713.979049	56.731674
2688.365799	166619.131871	56.736679
2687.826364	166521.548424	56.741684
2687.344406	166414.495721	56.746689
2686.315964	166322.407110	56.751693
2685.834406	166214.757286	56.756698
2685.033432	166116.021076	56.761703
2684.633234	166020.298779	56.766708
2683.885586	165915.883557	56.771713
2683.297189	165816.783866	56.776717
2682.555580	165707.612718	56.781722
2681.997759	165613.518578	56.786727
2681.075478	165512.107548	56.791732
2680.845108	165404.432999	56.796737
2680.103369	165306.121886	56.801741
2679.426478	165197.183583	56.806746
2678.735807	165097.237394	56.811751
2678.065015	164989.710120	56.816756
2677.510527	164878.706237	56.821761
2676.746703	164772.580281	56.826765
2676.149196	164674.820182	56.831770
2675.587747	164561.860250	56.836775
2674.596946	164454.817552	56.841780
2674.179575	164367.646699	56.846785
2672.964750	164265.230125	56.851789
2672.438411	164157.923991	56.856794
2671.956421	164057.273694	56.861799
2671.102729	163959.695959	56.866804
2670.756904	163856.761418	56.871809
2669.868435	163755.566046	56.876813
2669.354257	163654.260800	56.881818
2668.633814	163548.195106	56.886823
2667.927263	163451.752454	56.891828
2667.341265	163352.264899	56.896833
2666.704192	163258.202089	56.901837
2665.928201	163149.336458	56.906842
2665.411135	163046.177057	56.911847
2664.586102	162941.541015	56.916852
2664.000110	162841.444574	56.921857
2663.584697	162754.493429	56.926861
2662.742891	162643.999602	56.931866
2662.005380	162546.330988	56.936871
2661.259033	162452.046023	56.941876
2660.984737	162349.040869	56.946881
2659.955587	162248.965431	56.951885
2659.334487	162142.023573	56.956890
2658.614861	162042.319240	56.961895
2657.755986	161943.972221	56.966900
2657.115972	161842.552150	56.971905
2657.070159	161753.815769	56.976909
2656.630548	161645.994805	56.981914
2655.698963	161535.188061	56.986919
2654.729480	161439.262884	56.991924
2654.360146	161317.586385	56.996929
2653.497598	161221.721136	57.001933
2652.941312	161127.384128	57.006938
2652.414879	161028.491131	57.011943
2651.471145	160917.993367	57.016948
2651.037684	160822.162926	57.021953
2649.996895	160718.571956	57.026957
2649.506844	160619.013231	57.031962
2648.499557	160519.117187	57.036967
2647.908022	160420.655750	57.041972
2647.601717	160314.267051	57.046977
2646.988127	160221.073037	57.051981
2646.305529	160117.935619	57.056986
2645.891346	160007.941621	57.061991
2645.224909	159912.862507	57.066996
2644.298404	159801.373875	57.072001
2643.566491	159714.162479	57.077005
2643.278482	159591.334848	57.082010
2642.489604	159494.712544	57.087015
2641.533287	159394.010697	57.092020
2641.255895	159288.891834	57.097025
2640.054775	159191.216934	57.102029
2639.575514	159084.757660	57.107034
2639.013839	158977.409147	57.112039
2638.427032	158874.984853	57.117044
2637.833181	158766.968301	57.122049
2636.965291	158671.237988	57.127053
2636.274306	158569.632011	57.132058
2635.865857	158463.519376	57.137063
2634.946272	158367.302294	57.142068
2634.549207	158255.836423	57.147073
2633.769216	158159.597801	57.152077
2632.936302	158054.087606	57.157082
2632.489720	157945.707037	57.162087
2631.588404	157845.623884	57.167092
2631.445840	157743.971575	57.172097
2630.728440	157646.148114	57.177101
2629.967323	157536.992354	57.182106
2629.597340	157424.558728	57.187111
2628.488074	157321.764166	57.192116
2628.318465	157201.036485	57.197121
2627.410181	157105.927108	57.202125
2626.860486	156993.027589	57.207130
2625.756046	156889.839479	57.212135
2625.101102	156783.771072	57.217140
2624.270134	156676.027458	57.222145
2623.634656	156566.753183	57.227149
2623.265434	156463.208341	57.232154
2622.679683	156363.054092	57.237159
2621.717939	156263.925823	57.242164
2621.433134	156150.097282	57.247169
2620.777057	156058.294101	57.252173
2620.016488	155952.156034	57.257178
2619.386840	155846.595010	57.262183
2618.583980	155736.358401	57.267188
2618.020456	155633.215514	57.272193
2617.084552	155535.025950	57.277197
2616.321769	155425.394165	57.282202
2615.927274	155322.644927	57.287207
2615.132289	155229.912631	57.292212
2614.719262	155125.222057	57.297217
2614.150685	155014.124432	57.302221
2613.353537	154906.546331	57.307226
2612.650159	154802.652742	57.312231
2612.077851	154697.848908	57.317236
2611.427361	154586.397044	57.322241
2610.527543	154490.530983	57.327245
2610.045609	154388.306904	57.332250
2609.752086	154277.727426	57.337255
2608.737007	154178.867960	57.342260
2608.159132	154063.135370	57.347265
2607.231380	153958.962170	57.352269
2606.475991	153853.236656	57.357274
2605.979143	153751.741415	57.362279
2605.222342	153648.164939	57.367284
2604.816649	153544.927190	57.372289
2604.110943	153447.139437	57.377293
2603.510351	153335.836369	57.382298
2602.955665	153229.420069	57.387303
2602.044892	153123.975710	57.392308
2601.675065	153022.081246	57.397313
2600.795723	152905.307326	57.402317
2600.287230	152804.604888	57.407322
2599.570018	152702.397843	57.412327
2598.961101	152594.988034	57.417332
2598.467822	152478.751845	57.422337
2597.726031	152384.404795	57.427341
2596.971896	152279.370468	57.432346
2596.385137	152164.052644	57.437351
2594.950737	152058.961579	57.442356
2594.677319	151959.889530	57.447361
2593.815516	151861.025407	57.452365
2593.503661	151758.274069	57.457370
2593.083446	151645.829614	57.462375
2592.264890	151545.879219	57.467380
2591.912934	151430.717418	57.472385
2591.075882	151351.297425	57.477389
2590.839283	151159.552712	57.482394
2590.332148	151041.849442	57.487399
2589.203555	150936.344938	57.492404
2588.660425	150812.522008	57.497409
2588.261832	150719.256554	57.502413
2587.255792	150593.207326	57.507418
2586.706509	150477.470087	57.512423
2585.917914	150369.714758	57.517428
2585.402144	150266.377653	57.522433
2584.383596	150151.186197	57.527437
2583.849270	150049.708331	57.532442
2582.990252	149929.853381	57.537447
2582.419626	149818.341450	57.542452
2581.759496	149714.863759	57.547457
2581.229306	149597.754018	57.552461
2580.531091	149486.949759	57.557466
2579.662004	149385.514319	57.562471
2579.084349	149279.673730	57.567476
2578.480373	149168.690413	57.572481
2577.677270	149057.357758	57.577485
2577.272346	148947.474782	57.582490
2576.647434	148838.834409	57.587495
2575.891208	148730.914213	57.592500
2574.882517	148622.170174	57.597505
2574.320822	148513.444634	57.602509
2573.501457	148415.537485	57.607514
2573.114903	148308.487889	57.612519
2572.221569	148206.348328	57.617524
2571.959090	148099.546657	57.622529
2571.030172	148000.056834	57.627533
2570.518964	147876.773906	57.632538
2569.971395	147769.192453	57.637543
2569.554331	147670.868000	57.642548
2568.889353	147551.080166	57.647553
2568.270477	147450.869376	57.652557
2567.900767	147321.453361	57.657562
2566.693860	147209.225307	57.662567
2566.201070	147111.219593	57.667572
2565.512803	146979.847525	57.672577
2564.618393	146871.294707	57.677581
2563.711247	146767.039683	57.682586
2563.408317	146653.399524	57.687591
2562.362314	146550.069510	57.692596
2562.104689	146436.575452	57.697601
2561.108838	146332.310511	57.702605
2560.277114	146221.996279	57.707610
2559.542729	146103.025552	57.712615
2558.876527	146015.191737	57.717620
2558.464775	145914.508231	57.722625
2557.756278	145805.726307	57.727629
2556.991884	145697.855877	57.732634
2556.948219	145590.977184	57.737639
2556.215781	145484.093638	57.742644
2555.698583	145368.738417	57.747649
2554.524347	145266.589366	57.752653
2554.241165	145149.329841	57.757658
2553.736273	145040.353120	57.762663
2552.388396	144930.582721	57.767668
2552.108100	144807.084624	57.772673
2551.192272	144711.123124	57.777677
2550.688758	144599.453750	57.782682
2550.006449	144484.826882	57.787687
2549.342646	144381.557851	57.792692
2548.661738	144271.074141	57.797697
2547.690674	144168.807560	57.802701
2547.438503	144067.113579	57.807706
2547.125592	143959.914654	57.812711
2545.862021	143842.561299	57.817716
2545.749416	143732.612101	57.822721
2545.014185	143615.684163	57.827725
2544.424399	143509.725142	57.832730
2543.760451	143394.845276	57.837735
2542.957272	143277.726082	57.842740
2542.284966	143168.642719	57.847745
2541.396085	143063.850838	57.852749
2540.797567	142949.267235	57.857754
2540.390522	142835.924384	57.862759
2539.368749	142732.438075	57.867764
2538.900757	142615.166643	57.872769
2538.492616	142514.125144	57.877773
2537.686356	142394.849706	57.882778
2537.151276	142284.832882	57.887783
2536.375130	142170.585307	57.892788
2536.227742	142047.712547	57.897793
2534.939372	141938.095900	57.902797
2534.339451	141807.557687	57.907802
2533.800580	141710.186272	57.912807
2532.804224	141597.030370	57.917812
2532.279552	141488.158338	57.922817
2531.676907	141369.896559	57.927821
2530.879818	141262.428062	57.932826
2530.077124	141148.455374	57.937831
2529.684550	141035.752241	57.942836
2529.272679	140924.158000	57.947841
2528.126905	140826.148676	57.952845
2527.587050	140704.055096	57.957850
2527.387249	140598.730525	57.962855
2526.446508	140486.408556	57.967860
2526.009464	140364.211121	57.972865
2525.011472	140249.256338	57.977869
2524.365483	140139.836653	57.982874
2523.616554	140028.235629	57.987879
2523.122366	139927.000422	57.992884
2522.764756	139803.242618	57.997889
2521.668480	139684.087387	58.002893
2521.195264	139575.468232	58.007898
2520.938710	139458.010385	58.012903
2519.819939	139359.836416	58.017908
2519.217766	139225.955588	58.022913
2518.715565	139123.136232	58.027917
2518.097103	139007.694107	58.032922
2517.435850	138892.081341	58.037927
2516.307277	138779.427121	58.042932
2515.801502	138661.414783	58.047937
2515.122691	138544.294270	58.052941
2514.444202	138441.695788	58.057946
2514.061915	138322.242288	58.062951
2513.412056	138218.153585	58.067956
2512.564484	138095.471514	58.072961
2511.821269	137991.576271	58.077965
2511.251710	137860.224668	58.082970
2510.775645	137764.113910	58.087975
2509.860828	137637.086748	58.092980
2509.289402	137531.704885	58.097985
2508.655465	137418.532811	58.102989
2507.967663	137303.222676	58.107994
2507.305030	137184.161240	58.112999
2506.179052	137067.092065	58.118004
2505.794721	136960.780599	58.123009
2505.113339	136857.019316	58.128013
2504.773798	136732.852256	58.133018
2504.055214	136612.963542	58.138023
2503.479259	136523.237408	58.143028
2503.154180	136405.294410	58.148033
2502.051154	136281.008905	58.153037
2501.369871	136159.629787	58.158042
2501.109276	136048.995425	58.163047
2500.105250	135935.366897	58.168052
2499.594272	135805.971607	58.173057
2499.075878	135700.943647	58.178061
2498.434463	135581.059657	58.183066
2497.547286	135461.672442	58.188071
2496.980870	135345.042351	58.193076
2496.687833	135223.580205	58.198081
2495.517293	135103.553396	58.203085
2494.833513	134976.640952	58.208090
2494.329196	134864.690485	58.213095
2493.555616	134743.852763	58.218100
2492.957788	134620.472464	58.223105
2491.948685	134514.014919	58.228109
2491.534751	134381.384032	58.233114
2491.073458	134278.638748	58.238119
2490.378537	134166.772019	58.243124
2489.771818	134037.514158	58.248129
2488.933980	133922.838284	58.253133
2487.801053	133819.680282	58.258138
2487.584327	133701.375466	58.263143
2486.986070	133583.068099	58.268148
2486.287398	133464.421464	58.273153
2485.681916	133352.696174	58.278157
2485.230219	133222.325002	58.283162
2484.410862	133110.316998	58.288167
2483.255056	132993.142056	58.293172
2482.997855	132874.935999	58.298177
2482.267850	132757.554812	58.303181
2481.468852	132645.977291	58.308186
2481.013459	132516.232353	58.313191
2480.427346	132403.948822	58.318196
2480.004449	132279.966607	58.323201
2478.966330	132161.391917	58.328205
2478.325393	132052.827476	58.333210
2477.921517	131934.407249	58.338215
2476.769024	131816.055370	58.343220
2476.375805	131688.997178	58.348225
2475.532135	131577.049900	58.353229
2474.794019	131457.655807	58.358234
2474.407788	131354.388421	58.363239
2473.525839	131239.222321	58.368244
2473.404108	131114.511601	58.373249
2472.627172	131000.841324	58.378253
2471.820679	130875.097067	58.383258
2471.059121	130757.513278	58.388263
2470.433388	130640.975371	58.393268
2469.816188	130525.884550	58.398273
2469.096902	130406.758673	58.403277
2468.440415	130281.844292	58.408282
2468.107764	130166.163695	58.413287
2467.323791	130046.338345	58.418292
2466.539459	129926.437361	58.423297
2465.703211	129814.597564	58.428301
2465.237704	129696.526784	58.433306
2464.678767	129568.183582	58.438311
2464.206379	129459.919995	58.443316
2463.424990	129328.095028	58.448321
2462.720631	129203.281983	58.453325
2462.112583	129090.634187	58.458330
2461.686714	128965.638361	58.463335
2460.786351	128834.152120	58.468340
2460.222648	128713.687983	58.473345
2459.536648	128592.329324	58.478349
2458.928240	128471.505017	58.483354
2458.631453	128349.641217	58.488359
2457.832182	128215.601831	58.493364
2457.118124	128087.417093	58.498369
2456.132272	127968.674159	58.503373
2455.328780	127846.677003	58.508378
2454.625422	127717.298486	58.513383
2454.156307	127597.268744	58.518388
2453.410933	127474.705231	58.523393
2452.838225	127357.944144	58.528397
2452.060772	127230.891049	58.533402
2451.891904	127105.177148	58.538407
2451.113073	126992.717416	58.543412
2450.448923	126859.577626	58.548417
2449.913445	126727.040368	58.553421
2449.134870	126611.089783	58.558426
2448.187701	126466.948179	58.563431
2447.507900	126348.176475	58.568436
2447.291911	126227.020484	58.573441
2446.117811	126098.740212	58.578445
2445.354941	125977.773619	58.583450
2444.823753	125855.640612	58.588455
2444.033399	125722.602594	58.593460
2443.466342	125604.222649	58.598465
2442.944046	125487.372707	58.603469
2442.171178	125362.219778	58.608474
2441.456544	125237.553455	58.613479
2440.920330	125118.065949	58.618484
2440.532930	125004.257135	58.623489
2439.686393	124870.800464	58.628493
2439.337684	124750.853106	58.633498
2438.637299	124614.618928	58.638503
2437.646611	124497.187204	58.643508
2437.204963	124366.259359	58.648513
2436.171449	124241.267251	58.653517
2435.613850	124118.612973	58.658522
2435.284037	123996.291399	58.663527
2434.154717	123865.932150	58.668532
2433.798249	123730.905074	58.673537
2433.055381	123616.612477	58.678541
2431.865170	123507.330836	58.683546
2431.679678	123379.376660	58.688551
2430.602717	123265.938505	58.693556
2430.389619	123135.462982	58.698561
2429.964694	123011.726137	58.703565
2429.314601	122883.086126	58.708570
2428.774951	122758.898828	58.713575
2427.473736	122642.337156	58.718580
2427.223929	122508.150118	58.723585
2426.379591	122387.123775	58.728589
2425.576751	122271.944947	58.733594
2425.603006	122141.131629	58.738599
2424.447302	122011.534817	58.743604
2424.140928	121883.111822	58.748609
2423.386723	121756.106352	58.753613
2422.298465	121630.538444	58.758618
2421.984762	121509.482795	58.763623
2421.408914	121392.722775	58.768628
2420.838581	121251.368310	58.773633
2419.890176	121126.936064	58.778637
2419.037639	120998.426211	58.783642
2418.610214	120872.922224	58.788647
2417.459671	120755.595912	58.793652
2417.240368	120621.451738	58.798657
2416.704343	120496.855538	58.803661
2415.908868	120366.244800	58.808666
2415.723409	120243.289225	58.813671
2414.568261	120124.861881	58.818676
2414.133459	119989.326765	58.823681
2413.396172	119871.139044	58.828685
2412.652157	119736.295430	58.833690
2412.243128	119608.566410	58.838695
2411.290402	119493.283902	58.843700
2410.730092	119344.942594	58.848705
2410.045599	119226.743087	58.853709
2409.483751	119096.355609	58.858714
2409.053826	118975.323784	58.863719
2407.934277	118838.030589	58.868724
2407.388620	118698.742779	58.873729
2407.025464	118573.988740	58.878733
2406.339864	118454.377370	58.883738
2405.694771	118317.741724	58.888743
2405.021589	118193.692495	58.893748
2404.254226	118051.212325	58.898753
2403.870199	117924.998413	58.903757
2402.869788	117803.999050	58.908762
2402.210623	117678.096571	58.913767
2401.294611	117543.532882	58.918772
2401.060933	117406.246531	58.923777
2400.157631	117276.169954	58.928781
2399.581274	117155.976033	58.933786
2398.943202	117011.259520	58.938791
2398.115993	116886.447601	58.943796
2397.611025	116755.529790	58.948801
2396.623992	116629.328998	58.953805
2395.948653	116498.636285	58.958810
2395.660575	116370.726436	58.963815
2394.860168	116247.182859	58.968820
2394.247823	116105.368112	58.973825
2393.882839	115985.952296	58.978829
2393.082885	115854.248056	58.983834
2392.340419	115713.509758	58.988839
2391.704084	115583.710513	58.993844
2391.112130	115461.610242	58.998849
2390.285320	115344.396936	59.003853
2389.542594	115209.075512	59.008858
2389.212473	115063.089952	59.013863
2388.540500	114934.232697	59.018868
2387.988943	114792.790135	59.023873
2387.400773	114668.109911	59.028877
2386.450767	114533.396195	59.033882
2385.795095	114404.843712	59.038887
2385.045412	114271.990986	59.043892
2384.719903	114125.908577	59.048897
2384.132491	114011.970169	59.053901
2383.295521	113862.143321	59.058906
2382.723188	113733.485865	59.063911
2381.902419	113597.842768	59.068916
2381.287364	113465.239532	59.073921
2380.494752	113325.664923	59.078925
2379.757845	113195.360844	59.083930
2379.291130	113059.689923	59.088935
2378.258021	112936.719903	59.093940
2377.886887	112796.110430	59.098945
2377.251178	112666.110396	59.103949
2376.558621	112533.581521	59.108954
2376.177794	112392.055651	59.113959
2375.254225	112262.382606	59.118964
2374.758636	112134.273365	59.123969
2374.123974	111993.348482	59.128973
2373.211064	111860.661409	59.133978
2372.447959	111732.660122	59.138983
2371.448550	111599.931048	59.143988
2371.128000	111468.256384	59.148993
2370.693991	111333.662201	59.153997
2369.895534	111206.176931	59.159002
2369.065580	111085.214617	59.164007
2368.346043	110957.426209	59.169012
2367.904999	110811.654471	59.174017
2367.338377	110686.952710	59.179021
2366.468077	110555.344707	59.184026
2365.898993	110423.143913	59.189031
2365.071640	110296.410403	59.194036
2364.689557	110145.613779	59.199041
2364.082129	110035.935772	59.204045
2363.186819	109904.798466	59.209050
2363.101439	109753.995285	59.214055
2362.040097	109639.054366	59.219060
2361.251176	109489.094112	59.224065
2360.795121	109356.747907	59.229069
2360.141735	109225.582239	59.234074
2359.345683	109095.188661	59.239079
2358.537566	108972.469299	59.244084
2358.169564	108824.724403	59.249089
2357.523869	108701.282667	59.254093
2356.695128	108554.266040	59.259098
2356.209254	108420.305263	59.264103
2355.514931	108292.520464	59.269108
2354.790117	108150.381988	59.274113
2354.205712	108024.630676	59.279117
2353.178426	107873.817184	59.284122
2353.022336	107742.771044	59.289127
2352.198862	107612.795882	59.294132
2351.763480	107472.284256	59.299137
2350.962204	107347.395713	59.304141
2349.818237	107200.488069	59.309146
2349.570196	107074.548792	59.314151
2348.876948	106945.197425	59.319156
2348.053667	106808.107626	59.324161
2347.367548	106676.707192	59.329165
2346.453689	106543.903325	59.334170
2346.000550	106414.726126	59.339175
2345.405670	106291.180821	59.344180
2345.042892	106147.455015	59.349185
2344.351496	106014.713983	59.354189
2343.602913	105875.612779	59.359194
2342.741222	105736.225783	59.364199
2342.388791	105607.423999	59.369204
2341.482784	105469.650755	59.374209
2340.680175	105342.520597	59.379213
2340.453707	105198.912129	59.384218
2339.810115	105064.322589	59.389223
2338.678624	104936.130144	59.394228
2338.221205	104801.626773	59.399233
2337.183675	104665.300178	59.404237
2336.689153	104551.442045	59.409242
2336.140244	104411.378807	59.414247
2335.492039	104282.567669	59.419252
2334.859983	104144.898258	59.424257
2334.471402	104010.363093	59.429261
2333.522539	103887.679432	59.434266
2333.375641	103735.896063	59.439271
2332.572818	103621.659906	59.444276
2332.185351	103471.718080	59.449281
2331.332707	103333.733124	59.454285
2330.594094	103203.375274	59.459290
2329.776078	103047.896431	59.464295
2329.044086	102921.878283	59.469300
2328.384402	102788.674542	59.474305
2327.697127	102647.971298	59.479309
2326.810720	102506.266453	59.484314
2326.381334	102370.560878	59.489319
2325.645100	102235.399549	59.494324
2325.227742	102098.329769	59.499329
2324.645807	101962.828373	59.504333
2323.512634	101828.043181	59.509338
2323.184141	101694.279341	59.514343
2322.478944	101558.311397	59.519348
2322.064153	101413.626773	59.524353
2321.303284	101285.249614	59.529357
2320.563295	101142.096252	59.534362
2320.066486	101001.233197	59.539367
2318.999742	100867.597525	59.544372
2318.697630	100725.094091	59.549377
2317.812899	100588.443519	59.554381
2316.899985	100455.185457	59.559386
2316.598372	100307.565607	59.564391
2315.644785	100184.147358	59.569396
2315.478158	100039.216305	59.574401
2314.829988	99909.909172	59.579405
2313.574743	99771.742788	59.584410
2313.341013	99622.391279	59.589415
2312.574926	99493.270101	59.594420
2312.002034	99352.283289	59.599425
2311.549679	99218.394842	59.604429
2310.897860	99075.303753	59.609434
2310.361433	98934.624520	59.614439
2309.355051	98794.540773	59.619444
2308.665304	98650.272274	59.624449
2308.197590	98518.458053	59.629453
2307.248066	98383.993694	59.634458
2307.143188	98229.157197	59.639463
2306.076098	98097.472166	59.644468
2305.472431	97951.367799	59.649473
2305.064773	97814.702495	59.654477
2304.160300	97670.055648	59.659482
2303.490509	97532.418830	59.664487
2302.628707	97395.529973	59.669492
2302.145933	97244.762079	59.674497
2301.077887	97117.091182	59.679501
2300.451839	96986.217879	59.684506
2300.322391	96827.437305	59.689511
2299.462537	96702.608715	59.694516
2298.810735	96565.215918	59.699521
2297.825344	96432.170403	59.704525
2296.968514	96287.810220	59.709530
2296.754331	96153.838617	59.714535
2295.883112	96016.940573	59.719540
2295.533046	95873.568120	59.724545
2294.971909	95735.500106	59.729549
2294.458957	95605.549123	59.734554
2293.710812	95456.300205	59.739559
2292.970075	95326.412327	59.744564
2292.106189	95171.583931	59.749569
2291.470786	95037.489184	59.754573
2290.904245	94885.799105	59.759578
2290.204228	94760.385209	59.764583
2289.457977	94613.925541	59.769588
2289.178492	94477.837205	59.774593
2288.267751	94331.646449	59.779597
2287.434877	94191.658860	59.784602
2287.212871	94056.470796	59.789607
2286.201890	93915.549303	59.794612
2285.341500	93773.596559	59.799617
2284.796650	93640.256799	59.804621
2283.832104	93498.893039	59.809626
2283.312808	93365.531851	59.814631
2282.461123	93234.132852	59.819636
2282.146172	93083.176081	59.824641
2281.639907	92955.040337	59.829645
2280.481227	92836.444203	59.834650
2280.288626	92681.063775	59.839655
2279.684947	92555.158789	59.844660
2279.200151	92410.111575	59.849665
2278.508941	92268.965959	59.854669
2277.586091	92131.269330	59.859674
2277.155449	91985.918300	59.864679
2276.281123	91847.714828	59.869684
2275.709104	91705.070196	59.874689
2274.964825	91567.000041	59.879693
2274.191872	91434.324808	59.884698
2273.797210	91291.255277	59.889703
2272.998644	91151.230776	59.894708
2272.049260	91023.854974	59.899713
2271.577373	90879.265984	59.904718
2271.060387	90735.629820	59.909722
2270.488615	90595.148102	59.914727
2269.775313	90459.483009	59.919732
2269.085726	90318.463807	59.924737
2268.621951	90174.081084	59.929742
2267.759307	90033.249678	59.934746
2267.585857	89885.082114	59.939751
2266.516568	89749.167232	59.944756
2265.749674	89610.517054	59.949761
2265.188086	89462.134962	59.954766
2264.542137	89318.674409	59.959770
2264.109850	89170.907799	59.964775
2263.151645	89035.797620	59.969780
2262.862991	88891.883811	59.974785
2262.211134	88748.662542	59.979790
2260.922558	88604.452761	59.984794
2260.738142	88462.940727	59.989799
2259.797642	88333.487170	59.994804
2259.030624	88180.746694	59.999809
2258.343961	88052.864835	60.004814
2257.916410	87902.329395	60.009818
2257.329004	87759.440466	60.014823
2256.693442	87612.788132	60.019828
2256.043198	87470.297799	60.024833
2255.335020	87323.265912	60.029838
2254.792601	87193.331341	60.034842
2254.253381	87044.207939	60.039847
2253.398683	86893.373293	60.044852
2252.588732	86744.618217	60.049857
2251.957865	86613.350937	60.054862
2251.151223	86463.963370	60.059866
2250.973924	86319.186984	60.064871
2250.009331	86186.434855	60.069876
2249.582001	86031.874533	60.074881
2248.692758	85887.898601	60.079886
2247.705029	85749.061117	60.084890
2247.368360	85602.489261	60.089895
2246.710196	85464.596570	60.094900
2245.814593	85307.212587	60.099905
2245.410212	85177.788175	60.104910
2244.650490	85036.599200	60.109914
2244.284039	84882.772865	60.114919
2243.356428	84757.072405	60.119924
2242.844999	84610.839368	60.124929
2242.111182	84467.228739	60.129934
2241.107341	84325.443034	60.134938
2240.915798	84174.211910	60.139943
2239.771123	84043.111729	60.144948
2239.302570	83893.067471	60.149953
2238.607412	83760.775859	60.154958
2238.051524	83620.812669	60.159962
2237.713682	83484.802586	60.164967
2236.953778	83334.612031	60.169972
2236.570319	83189.135480	60.174977
2235.663281	83043.584525	60.179982
2234.551623	82888.731054	60.184986
2234.196435	82747.835505	60.189991
2233.597020	82605.249368	60.194996
2233.175429	82458.313522	60.200001
2232.349249	82309.421090	60.205006
2231.300588	82162.700862	60.210010
2231.179229	82006.828566	60.215015
2230.206140	81879.092756	60.220020
2229.726299	81724.388537	60.225025
2229.229747	81590.640470	60.230030
2227.908685	81440.070864	60.235034
2227.397052	81283.657464	60.240039
2226.690455	81149.476569	60.245044
2226.280867	81008.721804	60.250049
2225.701269	80864.864255	60.255054
2224.993935	80717.472676	60.260058
2224.487268	80577.255905	60.265063
2223.486113	80429.139822	60.270068
2222.815253	80291.365551	60.275073
2222.551476	80147.988883	60.280078
2221.543890	80006.524612	60.285082
2220.571178	79858.382762	60.290087
2220.231389	79716.681478	60.295092
2219.881875	79572.878805	60.300097
2218.896164	79445.077627	60.305102
2217.872466	79287.537494	60.310106
2217.557664	79142.914849	60.315111
2216.744614	79016.083850	60.320116
2215.990020	78866.171902	60.325121
2215.324382	78716.189908	60.330126
2214.611561	78592.178181	60.335130
2213.994891	78443.470441	60.340135
2213.548665	78299.685683	60.345140
2213.023420	78160.261393	60.350145
2212.364939	78029.394565	60.355150
2211.520316	77883.109612	60.360154
2211.139755	77737.753265	60.365159
2210.207017	77593.410659	60.370164
2209.651648	77449.142283	60.375169
2209.101021	77308.916774	60.380174
2208.538797	77173.173848	60.385178
2207.870416	77020.556158	60.390183
2207.234148	76869.176421	60.395188
2206.859199	76729.060105	60.400193
2206.050582	76581.910735	60.405198
2205.078261	76428.388951	60.410202
2204.861264	76288.415362	60.415207
2204.197674	76149.774441	60.420212
2203.500833	75991.682033	60.425217
2203.002738	75843.620748	60.430222
2202.093316	75695.853883	60.435226
2201.497114	75518.114403	60.440231
2200.611403	75393.053521	60.445236
2199.923205	75243.100724	60.450241
2199.368421	75096.156330	60.455246
2198.472617	74955.235260	60.460250
2198.001003	74788.911922	60.465255
2197.284954	74652.500731	60.470260
2196.525060	74508.950995	60.475265
2195.945612	74361.990538	60.480270
2195.281183	74216.596810	60.485274
2194.608992	74072.371071	60.490279
2194.282401	73922.655863	60.495284
2193.660036	73771.531584	60.500289
2192.992097	73620.878146	60.505294
2191.992340	73468.567986	60.510298
2191.385417	73315.265416	60.515303
2190.752745	73181.030306	60.520308
2189.964938	73023.102403	60.525313
2189.102313	72884.395239	60.530318
2188.260869	72734.181462	60.535322
2188.027640	72592.677817	60.540327
2187.091037	72466.325649	60.545332
2186.604981	72299.518531	60.550337
2186.014907	72160.013016	60.555342
2185.408964	72012.757335	60.560346
2184.746778	71859.075672	60.565351
2184.055090	71717.055538	60.570356
2183.129664	71570.075540	60.575361
2182.471484	71425.930106	60.580366
2181.849298	71282.742852	60.585370
2181.668514	71120.407376	60.590375
2180.673820	70988.632606	60.595380
2180.061911	70837.370642	60.600385
2179.754684	70683.952196	60.605390
2178.549510	70550.041097	60.610394
2178.271277	70398.210168	60.615399
2177.246834	70244.224833	60.620404
2176.724023	70103.253669	60.625409
2176.528510	69961.382836	60.630414
2175.505676	69806.228886	60.635418
2175.135149	69663.957256	60.640423
2174.461199	69513.855432	60.645428
2173.659627	69362.622246	60.650433
2173.331138	69215.267469	60.655438
2172.306137	69049.726112	60.660442
2171.619872	68907.712749	60.665447
2171.004540	68754.858634	60.670452
2170.181575	68609.892312	60.675457
2169.655439	68457.805410	60.680462
2169.030949	68307.622679	60.685466
2168.133574	68152.613976	60.690471
2167.393113	68007.974723	60.695476
2166.916229	67867.310082	60.700481
2166.365352	67720.318557	60.705486
2165.460825	67562.465712	60.710490
2164.990470	67418.155337	60.715495
2164.336345	67277.383761	60.720500
2163.512853	67117.083424	60.725505
2162.909430	66981.787262	60.730510
2161.754557	66834.261807	60.735514
2161.592771	66668.768473	60.740519
2160.350687	66542.446022	60.745524
2160.031202	66385.257265	60.750529
2159.806584	66253.259372	60.755534
2159.047272	66103.605923	60.760538
2158.262673	65961.107300	60.765543
2157.479814	65811.618177	60.770548
2156.949222	65667.624918	60.775553
2156.329582	65512.697827	60.780558
2155.336783	65371.528455	60.785562
2154.822930	65206.553155	60.790567
2154.112953	65076.321616	60.795572
2153.468000	64935.464391	60.800577
2153.034993	64790.122940	60.805582
2152.161205	64635.100788	60.810586
2151.687920	64495.945116	60.815591
2150.855819	64349.454539	60.820596
2150.202641	64201.765255	60.825601
2149.727978	64054.738993	60.830606
2148.947738	63914.461654	60.835610
2148.731813	63763.100298	60.840615
2148.024802	63612.229629	60.845620
2147.433396	63454.493866	60.850625
2146.645580	63295.802804	60.855630
2145.479944	63149.874591	60.860634
2145.126218	63015.348818	60.865639
2144.391583	62864.608777	60.870644
2143.935887	62717.555027	60.875649
2143.147147	62559.677560	60.880654
2142.579568	62418.234690	60.885658
2142.105486	62266.017652	60.890663
2141.631612	62115.359345	60.895668
2140.824854	61961.123992	60.900673
2140.142890	61799.804317	60.905678
2139.135283	61659.472117	60.910682
2138.870355	61497.012552	60.915687
2138.135012	61339.931391	60.920692
2137.376642	61191.570012	60.925697
2136.828053	61047.576633	60.930702
2135.545549	60895.644538	60.935706
2135.339854	60732.574400	60.940711
2134.530316	60589.477453	60.945716
2133.840917	60441.975232	60.950721
2133.111088	60292.793419	60.955726
2132.708450	60150.803309	60.960730
2132.189536	59983.696525	60.965735
2131.361701	59844.675676	60.970740
2130.874619	59690.420930	60.975745
2129.924574	59541.520617	60.980750
2129.494654	59394.770488	60.985754
2128.976811	59233.544987	60.990759
2128.023928	59092.707416	60.995764
2127.394573	58939.044870	61.000769
2127.234488	58784.176014	61.005774
2126.057094	58619.594621	61.010778
2125.616185	58477.056775	61.015783
2124.425263	58327.387803	61.020788
2123.704629	58166.238553	61.025793
2123.036805	58019.802892	61.030798
2122.061645	57872.910748	61.035802
2122.151136	57726.892138	61.040807
2121.217402	57578.315156	61.045812
2120.572347	57435.415769	61.050817
2120.088496	57286.937496	61.055822
2119.470676	57133.316586	61.060826
2118.419809	56986.522628	61.065831
2117.876593	56843.260373	61.070836
2117.658353	56686.180765	61.075841
2116.966112	56525.699610	61.080846
2116.094211	56395.041339	61.085850
2115.677402	56229.762443	61.090855
2114.885582	56084.960011	61.095860
2114.181676	55932.210932	61.100865
2113.554714	55774.422291	61.105870
2112.542358	55616.718308	61.110874
2112.347304	55476.246980	61.115879
2111.200194	55325.209380	61.120884
2110.626647	55186.835145	61.125889
2110.094691	55025.325879	61.130894
2109.726862	54874.975314	61.135898
2109.097482	54729.613547	61.140903
2108.245333	54574.105112	61.145908
2107.454447	54431.084558	61.150913
2106.736181	54263.403020	61.155918
2106.021588	54120.695569	61.160922
2105.766474	53963.455323	61.165927
2104.929430	53817.497760	61.170932
2104.120520	53664.439422	61.175937
2103.802046	53516.601525	61.180942
2102.634542	53369.801349	61.185946
2102.219456	53218.820144	61.190951
2101.566189	53062.365992	61.195956
2100.906550	52909.340977	61.200961
2100.213823	52749.760118	61.205966
2099.472313	52617.371163	61.210970
2099.252605	52447.010619	61.215975
2098.347614	52307.508573	61.220980
2097.616931	52141.288297	61.225985
2097.243673	51995.496502	61.230990
2096.590924	51848.272662	61.235994
2095.611966	51690.660793	61.240999
2095.009561	51542.558222	61.246004
2094.528002	51392.659596	61.251009
2093.778881	51237.593801	61.256014
2093.107593	51089.831772	61.261018
2092.742303	50923.270550	61.266023
2091.851841	50769.310089	61.271028
2091.223910	50616.929136	61.276033
2090.588981	50461.450146	61.281038
2089.666972	50299.244596	61.286042
2088.907826	50149.451038	61.291047
2088.089917	49996.498098	61.296052
2087.645255	49843.696044	61.301057
2086.793207	49693.892582	61.306062
2086.106290	49556.171115	61.311066
2085.705996	49397.209566	61.316071
2085.011292	49253.854264	61.321076
2084.294721	49091.930807	61.326081
2083.751515	48948.297690	61.331086
2083.063079	48795.464233	61.336090
2082.793043	48638.507066	61.341095
2081.857715	48492.842525	61.346100
2081.437801	48335.601811	61.351105
2080.536126	48175.718487	61.356110
2079.708191	48034.314316	61.361114
2079.424864	47875.085294	61.366119
2078.638999	47726.638660	61.371124
2077.875979	47567.880763	61.376129
2077.249331	47403.712604	61.381134
2076.689789	47267.443783	61.386138
2075.593167	47109.596999	61.391143
2075.213672	46952.824001	61.396148
2074.340542	46802.716232	61.401153
2073.906693	46645.457997	61.406158
2073.065392	46508.806424	61.411162
2072.549777	46348.372342	61.416167
2071.836135	46205.807069	61.421172
2071.395972	46049.412337	61.426177
2070.624677	45894.548619	61.431182
2069.714428	45748.412556	61.436186
2069.139864	45598.213955	61.441191
2068.482999	45435.682046	61.446196
2067.966019	45286.071600	61.451201
2067.226868	45128.635053	61.456206
2066.482122	44987.156827	61.461210
2065.860782	44829.375363	61.466215
2065.143208	44667.919747	61.471220
2064.354060	44532.075512	61.476225
2064.076391	44370.574989	61.481230
2063.312708	44233.530409	61.486234
2062.861555	44072.044373	61.491239
2061.977871	43929.353905	61.496244
2061.370010	43758.664177	61.501249
2060.817887	43616.885072	61.506254
2059.842079	43460.582752	61.511258
2059.285793	43305.815465	61.516263
2058.755148	43159.539716	61.521268
2057.956347	43002.887715	61.526273
2057.217600	42851.170359	61.531278
2056.607950	42711.260941	61.536282
2055.963545	42551.144767	61.541287
2055.135012	42400.957193	61.546292
2054.389610	42246.896642	61.551297
2054.164464	42098.038968	61.556302
2053.351920	41952.295678	61.561306
2052.707379	41799.266649	61.566311
2052.227940	41643.964509	61.571316
2051.355358	41481.465977	61.576321
2050.948126	41336.969536	61.581326
2049.977404	41181.809615	61.586330
2049.646199	41019.906223	61.591335
2048.914357	40864.040925	61.596340
2047.930477	40720.124974	61.601345
2047.497523	40563.554134	61.606350
2046.781104	40416.725681	61.611354
2046.235438	40255.315705	61.616359
2045.767411	40103.943275	61.621364
2045.040924	39948.722586	61.626369
2044.195052	39795.661204	61.631374
2043.527396	39635.390982	61.636378
2043.419640	39489.936231	61.641383
2042.341420	39332.100572	61.646388
2041.668941	39174.173537	61.651393
2041.126264	39005.161624	61.656398
2040.176897	38855.762593	61.661402
2039.505292	38702.759274	61.666407
2038.808612	38546.653505	61.671412
2037.989873	38400.505225	61.676417
2037.360254	38249.295085	61.681422
2036.550934	38095.740548	61.686426
2036.063790	37939.150296	61.691431
2035.331543	37800.851237	61.696436
2034.914920	37642.036393	61.701441
2034.198149	37487.149660	61.706446
2033.491740	37345.837455	61.711450
2032.867086	37183.407023	61.716455
2032.265459	37047.118228	61.721460
2031.694840	36882.534035	61.726465
2030.896426	36727.464922	61.731470
2030.321476	36585.643506	61.736474
2029.717080	36421.192474	61.741479
2028.925172	36278.704722	61.746484
2028.232194	36115.225407	61.751489
2027.738011	35963.133923	61.756494
2026.890779	35819.185796	61.761498
2026.222904	35648.825454	61.766503
2025.547152	35503.484111	61.771508
2024.742290	35352.024361	61.776513
2024.110918	35200.475234	61.781518
2023.517393	35058.211359	61.786522
2023.225974	34883.490766	61.791527
2022.459524	34746.709487	61.796532
2021.660375	34587.873620	61.801537
2021.016343	34438.722995	61.806542
2019.951392	34281.653279	61.811546
2019.276297	34139.732586	61.816551
2018.647232	33979.132397	61.821556
2018.192812	33829.127464	61.826561
2017.514527	33683.962004	61.831566
2016.627899	33554.370034	61.836570
2016.194002	33391.339330	61.841575
2015.335878	33239.121857	61.846580
2014.586791	33094.170332	61.851585
2014.100015	32930.333979	61.856590
2013.070691	32800.942800	61.861594
2012.721295	32656.838731	61.866599
2012.187523	32525.620177	61.871604
2011.336230	32376.173350	61.876609
2011.187869	32216.365690	61.881614
2010.069832	32080.099919	61.886618
2009.825711	31912.229431	61.891623
2008.920076	31774.172195	61.896628
2008.139763	31624.303765	61.901633
2007.757645	31463.187920	61.906638
2006.742445	31323.691835	61.911642
2006.102508	31169.093437	61.916647
2005.402519	31030.158152	61.921652
2004.789511	30877.103534	61.926657
2004.471986	30743.899283	61.931662
2003.581427	30586.800705	61.936666
2002.869885	30439.869440	61.941671
2002.032906	30292.499623	61.946676
2001.054540	30147.074830	61.951681
2001.058562	30008.545233	61.956686
2000.135217	29862.565991	61.961690
1999.505962	29728.572622	61.966695
1998.768527	29572.355319	61.971700
1997.953601	29426.481268	61.976705
1997.336665	29280.066792	61.981710
1996.552259	29135.277474	61.986714
1996.074323	28998.019436	61.991719
1995.519874	28859.659322	61.996724
1994.471997	28727.506907	62.001729
1994.303956	28579.515581	62.006734
1993.474883	28437.697005	62.011738
1992.942193	28290.044237	62.016743
1992.193203	28147.667295	62.021748
1991.416257	28003.457184	62.026753
1990.754611	27850.765713	62.031758
1989.646897	27719.703667	62.036762
1989.112730	27576.807928	62.041767
1988.671076	27433.803986	62.046772
1987.360778	27298.476729	62.051777
1986.972831	27165.614659	62.056782
1986.316773	27033.752730	62.061786
1985.468324	26896.479677	62.066791
1984.767277	26774.908256	62.071796
1983.947444	26642.846467	62.076801
1983.432851	26508.306270	62.081806
1982.599137	26402.895400	62.086810
1982.171501	26256.745174	62.091815
1981.286563	26134.346895	62.096820
1980.516288	26005.042022	62.101825
1979.667949	25896.299150	62.106830
1979.057217	25774.875752	62.111834
1978.230156	25651.960980	62.116839
1977.218078	25527.425116	62.121844
1976.227781	25431.517926	62.126849
1975.668882	25301.921393	62.131854
1974.614829	25208.650011	62.136858
1973.974177	25105.213515	62.141863
1973.305296	25001.608426	62.146868
1972.381743	24897.362099	62.151873
1971.819546	24817.603105	62.156878
1970.818309	24724.646008	62.161882
1969.969276	24628.262388	62.166887
1969.053439	24545.971388	62.171892
1968.698168	24455.194036	62.176897
1967.977336	24363.751850	62.181902
1967.212650	24287.104350	62.186906
1966.719875	24201.155618	62.191911
1965.994188	24123.934129	62.196916
1964.905737	24032.492968	62.201921
1964.539998	23952.616305	62.206926
1963.329967	23868.033292	62.211930
1963.118851	23787.272162	62.216935
1962.511616	23706.736987	62.221940
1961.969373	23631.666697	62.226945
1961.477188	23546.102820	62.231950
1960.307902	23469.533747	62.236954
1959.768782	23397.837509	62.241959
1959.019821	23316.733773	62.246964
1958.455177	23244.511631	62.251969
1957.514929	23163.240050	62.256974
1956.773987	23098.012836	62.261978
1956.409404	23015.800980	62.266983
1956.123002	22940.844960	62.271988
1955.439947	22863.223280	62.276993
1954.446505	22776.704749	62.281998
1953.986240	22704.433756	62.287002
1953.407231	22627.875343	62.292007
1952.597826	22555.023226	62.297012
1951.874560	22486.082156	62.302017
1951.370015	22403.752772	62.307022
1950.757735	22329.084309	62.312026
1950.131567	22256.792739	62.317031
1949.399833	22168.967891	62.322036
1948.248041	22105.266007	62.327041
1947.978257	22027.566251	62.332046
1947.000646	21954.486987	62.337050
1946.252946	21884.037205	62.342055
1945.569554	21810.742146	62.347060
1945.012763	21746.007670	62.352065
1944.878526	21669.539641	62.357070
1943.650702	21602.246668	62.362074
1943.284956	21529.327286	62.367079
1942.447532	21466.669269	62.372084
1941.880028	21395.163481	62.377089
1941.565168	21318.579755	62.382094
1940.691456	21256.784213	62.387098
1940.325854	21175.572983	62.392103
1939.661723	21099.902423	62.397108
1939.008121	21030.062110	62.402113
1938.375039	20951.537880	62.407118
1937.609932	20877.051358	62.412122
1937.058399	20798.181767	62.417127
1936.090603	20733.382872	62.422132
1935.558711	20663.966214	62.427137
1934.832507	20578.472141	62.432142
1934.083512	20510.717821	62.437146
1933.517958	20440.671933	62.442151
1932.848471	20368.816724	62.447156
1932.426887	20305.886534	62.452161
1932.038173	20214.310633	62.457166
1931.109124	20143.128471	62.462170
1930.654065	20066.216252	62.467175
1929.903344	19985.559426	62.472180
1929.055672	19906.833301	62.477185
1928.754143	19840.592586	62.482190
1927.743390	19766.934685	62.487194
1926.860115	19688.043603	62.492199
1926.161147	19623.580055	62.497204
1925.515723	19548.925327	62.502209
1924.946547	19476.339877	62.507214
1923.741665	19408.795328	62.512218
1923.664539	19332.324086	62.517223
1922.833753	19271.006402	62.522228
1922.067542	19198.958376	62.527233
1921.749005	19129.895169	62.532238
1920.639114	19061.570101	62.537242
1920.120570	18988.206021	62.542247
1919.986995	18918.876371	62.547252
1918.878289	18848.156905	62.552257
1918.596203	18778.005580	62.557262
1917.679782	18722.057951	62.562266
1917.121351	18643.201506	62.567271
1916.394651	18580.400907	62.572276
1915.298496	18508.753032	62.577281
1915.267030	18442.745752	62.582286
1914.493984	18383.613017	62.587290
1913.584317	18303.790187	62.592295
1912.702990	18238.897148	62.597300
1912.266755	18159.699313	62.602305
1911.583176	18103.149771	62.607310
1910.680705	18031.741351	62.612314
1910.186243	17953.683033	62.617319
1909.669651	17902.937728	62.622324
1908.594670	17836.621885	62.627329
1908.287567	17769.575820	62.632334
1907.277111	17699.449867	62.637338
1906.981207	17642.813623	62.642343
1906.192690	17584.803942	62.647348
1905.723828	17519.618732	62.652353
1905.002657	17440.452434	62.657358
1904.105139	17393.960771	62.662362
1903.908710	17321.608008	62.667367
1902.973614	17259.279197	62.672372
1902.194943	17195.721459	62.677377
1901.745428	17123.640089	62.682382
1901.289139	17063.692103	62.687386
1900.879645	16985.099078	62.692391
1899.809851	16924.722931	62.697396
1898.910357	16848.310387	62.702401
1898.679546	16785.765912	62.707406
1897.999982	16728.220483	62.712410
1897.388390	16647.317164	62.717415
1896.515221	16593.871521	62.722420
1895.581396	16511.660863	62.727425
1895.088273	16447.840063	62.732430
1894.522586	16398.797005	62.737434
1893.596024	16318.668417	62.742439
1892.957417	16266.909721	62.747444
1892.311904	16207.580760	62.752449
1891.755643	16125.614327	62.757454
1890.907780	16071.827478	62.762458
1890.490082	15997.010636	62.767463
1889.683991	15934.061322	62.772468
1888.902962	15876.066152	62.777473
1888.755191	15818.356922	62.782478
1887.534655	15760.121679	62.787482
1887.292466	15691.215286	62.792487
1886.465350	15627.808840	62.797492
1885.563259	15557.342257	62.802497
1884.864779	15493.734019	62.807502
1884.080091	15443.814810	62.812506
1883.550682	15374.711947	62.817511
1883.102876	15321.295248	62.822516
1882.436841	15258.305554	62.827521
1881.847613	15197.125110	62.832526
1880.912377	15135.255191	62.837530
1880.504069	15071.766107	62.842535
1879.559934	15014.065077	62.847540
1879.124238	14951.650648	62.852545
1878.627943	14885.273209	62.857550
1877.855009	14834.397573	62.862554
1877.289756	14765.532316	62.867559
1876.912501	14690.463874	62.872564
1876.243695	14643.540934	62.877569
1875.070636	14562.061563	62.882574
1874.492950	14512.677011	62.887578
1874.302537	14432.535315	62.892583
1873.341263	14379.725969	62.897588
1872.525045	14315.493477	62.902593
1872.206238	14245.802133	62.907598
1871.023160	14191.998256	62.912602
1870.439134	14119.285253	62.917607
1870.087489	14056.444733	62.922612
1869.367109	14003.136772	62.927617
1868.646016	13935.990621	62.932622
1868.069577	13887.870186	62.937626
1867.457134	13812.214269	62.942631
1866.893462	13741.648459	62.947636
1865.922486	13688.075582	62.952641
1865.444115	13622.608617	62.957646
1864.579387	13566.033102	62.962650
1864.226925	13492.017647	62.967655
1863.264382	13427.564133	62.972660
1862.520937	13373.815966	62.977665
1861.684678	13295.900653	62.982670
1860.992105	13254.016382	62.987674
1860.515973	13189.537847	62.992679
1859.946263	13140.608059	62.997684
1858.984667	13088.449550	63.002689
1858.749713	13021.112076	63.007694
1858.032826	12957.635095	63.012698
1857.288154	12910.145778	63.017703
1856.921889	12838.421104	63.022708
1856.098002	12775.398061	63.027713
1855.354388	12717.616482	63.032718
1854.688743	12649.906926	63.037722
1854.148323	12574.672166	63.042727
1853.595577	12521.224811	63.047732
1852.306206	12458.344064	63.052737
1851.926556	12404.436815	63.057742
1851.094702	12345.450712	63.062746
1850.610325	12294.766391	63.067751
1849.577350	12238.313479	63.072756
1848.855888	12184.334238	63.077761
1848.314198	12117.901881	63.082766
1847.714964	12078.345089	63.087770
1847.255301	12011.998807	63.092775
1846.819829	11955.018092	63.097780
1845.595165	11900.529724	63.102785
1845.340864	11837.054020	63.107790
1844.687627	11784.205188	63.112794
1843.969780	11720.438231	63.117799
1843.544469	11668.599523	63.122804
1842.787648	11610.419080	63.127809
1842.500704	11547.291436	63.132814
1841.253630	11485.158811	63.137818
1840.935523	11423.863289	63.142823
1840.075698	11377.520475	63.147828
1839.692761	11315.594189	63.152833
1838.942170	11247.388554	63.157838
1838.096148	11185.126816	63.162842
1837.469067	11130.009608	63.167847
1836.891203	11078.667804	63.172852
1836.082718	11011.780642	63.177857
1835.612949	10944.027104	63.182862
1834.654894	10894.240707	63.187866
1834.180690	10836.324123	63.192871
1833.762774	10767.113519	63.197876
1832.704205	10709.230241	63.202881
1832.136930	10648.095781	63.207886
1831.454040	10591.782612	63.212890
1830.646847	10531.073729	63.217895
1830.124898	10481.481799	63.222900
1829.619462	10431.121293	63.227905
1829.127385	10359.280402	63.232910
1828.238391	10308.757131	63.237914
1827.591412	10236.612806	63.242919
1826.807821	10193.025363	63.247924
1826.067149	10128.558675	63.252929
1825.803138	10073.646473	63.257934
1825.137110	10012.974469	63.262938
1824.313473	9941.803224	63.267943
1823.492224	9882.564709	63.272948
1823.346833	9824.497243	63.277953
1822.572334	9756.605516	63.282958
1821.804531	9708.416924	63.287962
1821.096258	9640.911658	63.292967
1820.393378	9582.648831	63.297972
1819.763046	9530.104471	63.302977
1818.886262	9463.667781	63.307982
1818.254381	9415.968208	63.312986
1817.890777	9346.612717	63.317991
1817.132687	9293.697761	63.322996
1816.066232	9237.401266	63.328001
1815.727521	9167.018219	63.333006
1815.151646	9111.572876	63.338010
1814.319904	9054.645737	63.343015
1814.066607	8989.755879	63.348020
1812.783953	8935.326336	63.353025
1812.562967	8871.838503	63.358030
1811.627115	8815.403340	63.363034
1811.275234	8763.129868	63.368039
1810.539136	8694.980460	63.373044
1809.760635	8649.434297	63.378049
1809.315394	8570.780363	63.383054
1808.211672	8529.398355	63.388058
1807.561213	8457.712026	63.393063
1807.125465	8405.715033	63.398068
1806.161719	8353.683727	63.403073
1805.676846	8290.341241	63.408078
1805.032079	8233.670753	63.413082
1804.488740	8183.704848	63.418087
1803.561912	8124.875429	63.423092
1802.938555	8074.322261	63.428097
1802.671960	8010.348335	63.433102
1801.823949	7951.466854	63.438106
1801.305130	7897.316224	63.443111
1800.475868	7836.147667	63.448116
1799.884405	7770.860044	63.453121
1799.278919	7715.634422	63.458126
1798.462218	7670.263374	63.463130
1798.052963	7598.064041	63.468135
1797.148684	7546.164954	63.473140
1796.374030	7491.804781	63.478145
1796.002844	7425.338294	63.483150
1794.934851	7371.638858	63.488154
1794.194507	7311.931887	63.493159
1793.661405	7249.012467	63.498164
1793.077514	7200.894278	63.503169
1792.547143	7145.654112	63.508174
1791.788370	7094.001701	63.513178
1791.204118	7037.741079	63.518183
1790.820219	6976.263960	63.523188
1789.893145	6931.009329	63.528193
1789.397478	6861.744327	63.533198
1788.608482	6810.540225	63.538202
1787.741223	6744.915175	63.543207
1787.426610	6687.866852	63.548212
1786.548254	6636.581308	63.553217
1786.084844	6567.563395	63.558222
1785.028513	6513.100088	63.563226
1784.392121	6453.223884	63.568231
1783.553923	6411.356410	63.573236
1783.188103	6356.707517	63.578241
1782.900943	6290.402352	63.583246
1781.956017	6238.720959	63.588250
1781.493507	6187.010467	63.593255
1781.048985	6122.964851	63.598260
1779.799605	6072.065156	63.603265
1779.551566	6000.568133	63.608270
1778.760282	5955.408506	63.613274
1778.108309	5891.844061	63.618279
1777.559699	5840.096396	63.623284
1776.502897	5782.724557	63.628289
1776.109924	5712.072246	63.633294
1775.284305	5655.578351	63.638298
1775.058246	5602.997859	63.643303
1774.117196	5538.072933	63.648308
1773.133381	5490.722633	63.653313
1772.834736	5427.562334	63.658318
1771.985156	5375.710287	63.663322
1771.431781	5321.280353	63.668327
1770.584413	5260.496009	63.673332
1769.866251	5204.685588	63.678337
1769.584876	5152.036613	63.683342
1768.423387	5101.124740	63.688346
1768.126098	5040.899119	63.693351
1767.512454	4983.353542	63.698356
1766.664168	4917.786439	63.703361
1766.388158	4862.612992	63.708366
1765.252594	4810.993695	63.713370
1764.677742	4750.621683	63.718375
1763.959526	4690.592895	63.723380
1763.421195	4651.951942	63.728385
1762.639134	4586.754371	63.733390
1761.854536	4532.867254	63.738394
1761.127926	4479.987740	63.743399
1760.602445	4434.945149	63.748404
1760.288415	4380.850574	63.753409
1759.671614	4324.416170	63.758414
1758.411473	4269.627581	63.763418
1757.889338	4207.724133	63.768423
1757.520952	4152.732059	63.773428
1756.607138	4108.254521	63.778433
1756.049365	4042.571053	63.783438
1755.226772	3987.281848	63.788442
1754.765481	3937.603536	63.793447
1753.986210	3891.253529	63.798452
1753.421417	3835.602186	63.803457
1752.915841	3784.059962	63.808462
1751.990954	3727.827410	63.813466
1751.576026	3663.844561	63.818471
1750.812485	3618.544965	63.823476
1750.311371	3567.714933	63.828481
1749.769370	3514.837183	63.833486
1748.960812	3450.150440	63.838490
1748.076565	3391.413563	63.843495
1747.590081	3345.772711	63.848500
1746.753131	3293.677598	63.853505
1746.388517	3223.701476	63.858510
1745.592836	3175.573280	63.863514
1744.772415	3120.821684	63.868519
1744.388046	3062.147116	63.873524
1743.167467	3019.092999	63.878529
1742.677119	2954.483301	63.883534
1741.894108	2906.454133	63.888538
1741.167770	2856.442265	63.893543
1740.795219	2802.244516	63.898548
1739.788964	2756.971943	63.903553
1739.800622	2704.060455	63.908558
1738.896501	2661.241818	63.913562
1738.292613	2604.040756	63.918567
1737.729190	2548.907457	63.923572
1736.869836	2497.305298	63.928577
1736.434129	2443.138626	63.933582
1735.356926	2397.930484	63.938586
1734.629193	2335.177307	63.943591
1734.254938	2283.591915	63.948596
1733.406314	2235.028116	63.953601
1733.113996	2184.801372	63.958606
1731.816549	2138.467466	63.963610
1731.211836	2076.976482	63.968615
1730.431651	2030.984222	63.973620
1729.921923	1983.389404	63.978625
1729.432207	1937.161270	63.983630
1728.924447	1896.532451	63.988634
1728.088477	1853.077689	63.993639
1727.423887	1789.768797	63.998644
1726.828162	1742.027565	64.003649
1726.576596	1687.234381	64.008654
1725.688594	1634.422338	64.013658
1724.742590	1587.495810	64.018663
1724.406249	1533.181902	64.023668
1723.435903	1491.468550	64.028673
1722.598171	1430.857082	64.033678
1722.147479	1391.395505	64.038682
1721.411249	1338.527317	64.043687
1720.904551	1294.473128	64.048692
1720.157562	1247.355237	64.053697
1719.493096	1193.241375	64.058702
1718.813148	1149.544737	64.063706
1718.036979	1101.930465	64.068711
1717.453559	1053.006002	64.073716
1716.353229	1011.393529	64.078721
1716.140796	958.221180	64.083726
1715.605407	922.882385	64.088730
1714.997546	871.870546	64.093735
1714.113866	822.569553	64.098740
1713.243614	790.203245	64.103745
1712.519228	737.482027	64.108750
1711.378937	694.361352	64.113754
1710.715402	651.950409	64.118759
1710.454198	609.329034	64.123764
1709.639201	564.714172	64.128769
1709.291906	528.302529	64.133774
1708.556058	494.223480	64.138778
1708.013283	444.033857	64.143783
1707.311026	403.793344	64.148788
1706.477298	363.985401	64.153793
1705.822938	312.060420	64.158798
1705.336278	270.660115	64.163802
1704.183285	242.532958	64.168807
1703.755610	201.216522	64.173812
1702.725121	170.734651	64.178817
1702.449603	128.706726	64.183822
1701.355868	106.486947	64.188826
1700.897724	70.977124	64.193831
1700.529255	38.731495	64.198836
1699.004214	6.664905	64.203841
1698.839101	-24.367142	64.208846
1697.661180	-50.044022	64.213850
1696.743737	-64.780859	64.218855
1695.926733	-82.001443	64.223860
1690.808785	16.316290	64.228865
1690.945228	9.742678	64.233870
1691.431912	9.745815	64.238874
1691.948659	21.963465	64.243879
1692.168770	8.493456	64.248884
1691.583789	9.314908	64.253889
1691.011949	15.071501	64.258894
1689.780520	9.700705	64.263898
1688.564028	20.222543	64.268903
1688.398978	17.065043	64.273908
1687.504117	22.239038	64.278913
1686.386133	23.276033	64.283918
1685.684115	28.805738	64.288922
1685.830059	22.113921	64.293927
1685.081631	20.953960	64.298932
1684.597249	22.177311	64.303937
1683.845661	18.983670	64.308942
1683.111360	26.866485	64.313946
1682.487399	30.289688	64.318951
1682.065295	22.871270	64.323956
1681.210356	25.996859	64.328961
1680.497912	26.247228	64.333966
1679.872680	26.644587	64.338970
1679.504417	32.681077	64.343975
1678.609781	25.799742	64.348980
1678.189453	18.193395	64.353985
1677.098717	17.803715	64.358990
1676.898400	30.840132	64.363994
1676.269286	22.860110	64.368999
1675.526566	18.718931	64.374004
1674.244944	23.777752	64.379009
1674.198217	17.116541	64.384014
1674.092777	22.407989	64.389018
1672.944445	27.981782	64.394023
1672.009737	25.367563	64.399028
1670.757889	37.527112	64.404033
1671.078783	25.936500	64.409038
1670.523362	33.645834	64.414042
1669.560413	28.514660	64.419047
1668.506419	19.132472	64.424052
1667.782818	37.004747	64.429057
1668.104042	14.968792	64.434062
1667.184142	25.364685	64.439066
1665.651207	28.793508	64.444071
1665.714885	28.108503	64.449076
1665.064301	29.760363	64.454081
1664.099507	16.303529	64.459086
1663.576958	27.030529	64.464090
1662.648503	33.666914	64.469095
1662.272543	22.868210	64.474100
1661.506813	25.760448	64.479105
1661.302996	31.091179	64.484110
1660.384197	37.402771	64.489114
1659.553324	35.311357	64.494119
1659.243743	27.029858	64.499124
1658.327116	31.311650	64.504129
1657.742081	29.944401	64.509134
1656.877759	28.883278	64.514138
1656.333165	28.966649	64.519143
1655.795370	27.443669	64.524148
1655.154786	29.537048	64.529153
1654.859678	29.766861	64.534158
1653.660990	30.534427	64.539162
1653.427639	29.716839	64.544167
1652.835683	26.448966	64.549172
1651.194660	38.034856	64.554177
1651.309804	27.662745	64.559182
1650.443808	27.335143	64.564186
1649.294948	27.172317	64.569191
1649.572843	19.811441	64.574196
1648.375619	28.985155	64.579201
1647.957391	28.269472	64.584206
1647.366971	23.331434	64.589210
1646.568978	22.453736	64.594215
1646.130692	19.230839	64.599220
1645.404498	21.957534	64.604225
1645.173292	22.256042	64.609230
1644.105273	27.574247	64.614234
1642.928450	28.880793	64.619239
1642.135839	32.925281	64.624244
1641.914303	34.102156	64.629249
1641.447205	32.959016	64.634254
1640.557899	37.619659	64.639258
1639.889148	26.616744	64.644263
1639.546933	25.630378	64.649268
1639.065866	32.003321	64.654273
1638.526502	24.267663	64.659278
1637.693371	28.279165	64.664282
1636.288592	29.863189	64.669287
1635.644284	20.349708	64.674292
1634.943604	27.340983	64.679297
1635.257606	19.862413	64.684302
1634.454136	32.975720	64.689306
1633.643898	29.654220	64.694311
1633.140383	29.095584	64.699316
1632.301677	32.910864	64.704321
1630.766540	22.871873	64.709326
1630.341199	29.910871	64.714330
1630.284666	41.235608	64.719335
1629.693976	29.990068	64.724340
1628.285244	33.340837	64.729345
1628.084370	28.077581	64.734350
1627.313489	33.468435	64.739354
1626.663530	19.545305	64.744359
1626.550252	21.244277	64.749364
1625.633038	31.086271	64.754369
1625.133108	20.792952	64.759374
1624.777301	22.451608	64.764378
1623.497874	32.338528	64.769383
1622.568945	30.161784	64.774388
1621.693844	30.863768	64.779393
1621.251102	31.407185	64.784398
1620.875275	23.062105	64.789402
1620.445847	31.372723	64.794407
1620.155975	20.677046	64.799412
1619.305963	35.532324	64.804417
1618.814452	29.279225	64.809422
1617.228465	33.194300	64.814426
1616.609756	29.724113	64.819431
1616.119580	16.497821	64.824436
1615.346783	26.133953	64.829441
1615.282695	19.117552	64.834446
1614.538894	30.141469	64.839450
1613.960275	23.057002	64.844455
1613.728950	27.338743	64.849460
1612.429525	25.466856	64.854465
1611.716650	17.590047	64.859470
1611.207845	20.201795	64.864474
1610.629596	21.266613	64.869479
1609.446940	28.113698	64.874484
1608.328774	32.235143	64.879489
1608.384623	23.510842	64.884494
1607.553866	25.438909	64.889498
1606.842924	25.843594	64.894503
1606.351795	27.148452	64.899508
1605.458829	31.486423	64.904513
1605.167976	24.187515	64.909518
1604.898273	22.085816	64.914522
1604.697485	24.812628	64.919527
1603.557133	21.639774	64.924532
1602.518530	18.870209	64.929537
1601.932312	11.581963	64.934542
1601.133710	21.330999	64.939546
1600.722853	21.456209	64.944551
1599.575538	28.262992	64.949556
1598.222805	29.154399	64.954561
1598.451707	18.909299	64.959566
1597.585776	26.428283	64.964570
1597.015308	21.376708	64.969575
1596.630374	18.241535	64.974580
1595.881485	20.366325	64.979585
1595.757403	17.371052	64.984590
1595.248155	22.602078	64.989594
1593.747159	26.003790	64.994599
1593.177636	20.165201	64.999604
1592.382552	19.693894	65.004609
1592.257323	21.544570	65.009614
1591.749535	19.617886	65.014618
1590.642719	27.238217	65.019623
1589.989369	24.919938	65.024628
1589.116864	23.240424	65.029633
1588.722205	31.149722	65.034638
1588.245786	26.400160	65.039642
1587.303697	26.519888	65.044647
1586.663051	22.356214	65.049652
1585.705351	23.804583	65.054657
1585.062083	20.519651	65.059662
1584.445046	21.560676	65.064666
1583.991342	26.480118	65.069671
1583.881870	21.845718	65.074676
1583.005332	29.435776	65.079681
1582.298297	24.111024	65.084686
1581.600113	26.483218	65.089690
1580.844929	26.475487	65.094695
1580.435602	23.132889	65.099700
1579.310249	29.185593	65.104705
1578.773364	21.149952	65.109710
1577.953604	23.438964	65.114714
1577.366867	28.885724	65.119719
1577.125342	10.857754	65.124724
1576.412681	28.375065	65.129729
1575.412241	25.802865	65.134734
1574.600784	18.023730	65.139738
1573.501442	27.557217	65.144743
1573.653821	18.390249	65.149748
1572.798465	16.324834	65.154753
1572.655804	24.755463	65.159758
1571.787690	24.034003	65.164762
1570.784968	25.590451	65.169767
1570.169044	22.558211	65.174772
1569.368330	28.955138	65.179777
1569.067727	27.856520	65.184782
1568.928507	33.561751	65.189786
1567.277662	26.769070	65.194791
1566.639295	26.738054	65.199796
1565.830123	19.297588	65.204801
1565.459593	27.978879	65.209806
1565.258561	35.504195	65.214810
1564.685466	34.013651	65.219815
1563.484680	34.169759	65.224820
1562.410470	40.506072	65.229825
1561.844592	29.338612	65.234830
1561.221385	26.853132	65.239834
1560.930915	31.525881	65.244839
1560.933308	28.687125	65.249844
1560.178701	29.218604	65.254849
1559.125614	24.685246	65.259854
1558.408926	32.929551	65.264858
1557.453208	31.668527	65.269863
1557.461163	16.680574	65.274868
1556.331936	20.816408	65.279873
1555.388370	21.021535	65.284878
1554.839350	25.927741	65.289882
1554.209860	29.906911	65.294887
1554.028979	24.919598	65.299892
1553.630863	28.907736	65.304897
1552.378356	32.497061	65.309902
1551.519712	18.859421	65.314906
1550.854346	27.581250	65.319911
1550.754990	19.447718	65.324916
1550.096834	29.660135	65.329921
1548.936143	25.098149	65.334926
1548.334711	23.213160	65.339930
1547.535742	19.088845	65.344935
1547.486189	21.742747	65.349940
1546.756473	34.306633	65.354945
1546.060635	17.260711	65.359950
1545.120872	23.596160	65.364954
1544.317371	25.127272	65.369959
1543.969586	21.145726	65.374964
1543.306531	26.421698	65.379969
1542.209488	15.471111	65.384974
1541.446292	21.103599	65.389978
1540.738716	28.707820	65.394983
1540.672691	19.719051	65.399988
1540.037551	25.529882	65.404993
1539.564100	17.779054	65.409998
1538.605885	24.219934	65.415002
1537.612438	19.530462	65.420007
1537.171477	19.641543	65.425012
1536.605207	29.699020	65.430017
1536.514534	28.280056	65.435022
1535.448702	22.856219	65.440026
1534.201323	23.885453	65.445031
1533.969412	23.670018	65.450036
1533.393475	27.301653	65.455041
1532.871202	24.074777	65.460046
1531.546772	28.973314	65.465050
1530.973448	28.660747	65.470055
1530.412055	17.719665	65.475060
1529.844555	34.644668	65.480065
1529.802367	28.630844	65.485070
1529.295819	28.894268	65.490074
1527.715328	34.708666	65.495079
1527.018436	26.851420	65.500084
1526.346434	27.193172	65.505089
1526.236251	26.187299	65.510094
1525.752314	31.914188	65.515098
1524.560264	30.509388	65.520103
1524.090003	31.031963	65.525108
1523.119662	21.887281	65.530113
1522.685870	21.131517	65.535118
1522.132732	13.241976	65.540122
1521.068498	28.517639	65.545127
1520.324644	21.147234	65.550132
1519.324100	26.169345	65.555137
1519.194541	27.855138	65.560142
1518.746515	26.352616	65.565146
1518.057662	28.715459	65.570151
1518.032345	28.161282	65.575156
1517.050704	31.860541	65.580161
1516.260154	23.937761	65.585166
1515.500660	26.037451	65.590170
1515.060436	29.480374	65.595175
1514.242696	25.554586	65.600180
1512.985807	25.153532	65.605185
1512.622381	22.040185	65.610190
1512.043017	35.340244	65.615194
1511.765218	20.968532	65.620199
1511.371009	25.422810	65.625204
1510.101348	23.943622	65.630209
1509.549538	23.422646	65.635214
1508.893341	34.060519	65.640218
1508.161953	25.890231	65.645223
1507.241063	24.486504	65.650228
1506.398398	31.724285	65.655233
1505.677147	25.581837	65.660238
1504.995714	40.989068	65.665242
1504.687257	24.711042	65.670247
1504.593081	28.010673	65.675252
1504.107114	28.242447	65.680257
1503.363533	25.560078	65.685262
1502.549014	30.503752	65.690266
1501.605681	31.527264	65.695271
1501.039968	24.833423	65.700276
1500.088194	35.560843	65.705281
1499.498195	20.395112	65.710286
1498.653601	29.385117	65.715290
1497.983394	27.216192	65.720295
1497.864082	22.709514	65.725300
1497.292224	35.271977	65.730305
1496.224294	22.320447	65.735310
1495.581550	33.137525	65.740314
1494.772256	28.992791	65.745319
1494.695073	17.719322	65.750324
1493.844466	32.763938	65.755329
1492.887932	30.930660	65.760334
1492.446256	32.960931	65.765338
1491.793984	39.014185	65.770343
1491.316615	23.185611	65.775348
1490.061436	37.253780	65.780353
1489.678993	20.872407	65.785358
1488.851063	28.891560	65.790362
1488.004481	14.324831	65.795367
1488.200646	19.923145	65.800372
1487.413244	26.707466	65.805377
1486.366050	24.007121	65.810382
1485.926667	21.353685	65.815386
1485.011761	32.811652	65.820391
1484.674379	15.156888	65.825396
1483.415894	23.782177	65.830401
1482.855025	29.086076	65.835406
1482.231485	23.921546	65.840410
1481.854127	33.357679	65.845415
1481.912072	24.489558	65.850420
1480.426115	36.102928	65.855425
1480.034860	33.733566	65.860430
1479.300737	34.280735	65.865434
1478.515900	32.913742	65.870439
1477.461569	22.524075	65.875444
1476.576946	31.592985	65.880449
1476.144858	29.715793	65.885454
1475.658095	31.305396	65.890458
1475.451114	30.674438	65.895463
1475.206355	35.811417	65.900468
1473.864713	27.312361	65.905473
1473.270841	23.767309	65.910478
1472.629878	29.564887	65.915482
1472.193634	27.801893	65.920487
1471.302089	25.705995	65.925492
1470.392487	37.335006	65.930497
1470.065345	23.444210	65.935502
1469.605716	21.779546	65.940506
1468.610308	27.012160	65.945511
1468.223762	26.862305	65.950516
1467.546512	21.944425	65.955521
1466.725970	33.231289	65.960526
1465.792467	25.310746	65.965530
1464.799802	29.528991	65.970535
1464.925970	23.318116	65.975540
1464.207517	30.627627	65.980545
1463.566727	33.124764	65.985550
1462.266707	32.421519	65.990554
1461.550012	25.307003	65.995559
1461.177736	24.027410	66.000564
1460.891174	31.772887	66.005569
1460.373509	28.179458	66.010574
1459.362202	27.838745	66.015578
1458.622038	28.404226	66.020583
1458.233843	25.212827	66.025588
1457.316727	31.614089	66.030593
1456.390993	33.101577	66.035598
1455.987787	24.762464	66.040602
1455.256430	32.471402	66.045607
1455.186821	14.718903	66.050612
1454.212645	33.821559	66.055617
1453.492948	20.157152	66.060622
1452.746260	26.313719	66.065626
1451.869087	33.634266	66.070631
1451.501409	24.185690	66.075636
1450.769580	36.366745	66.080641
1450.001994	25.228229	66.085646
1449.210808	33.112250	66.090650
1448.834564	37.275113	66.095655
1448.855131	22.400279	66.100660
1447.546357	33.930313	66.105665
1446.721185	24.510293	66.110670
1446.174841	31.589037	66.115674
1445.546497	37.055049	66.120679
1444.785800	33.503400	66.125684
1443.754795	30.940842	66.130689
1443.498503	29.456746	66.135694
1442.873642	38.963757	66.140698
1442.629240	41.785817	66.145703
1441.367532	27.971017	66.150708
1440.543885	49.154910	66.155713
1440.117323	34.116171	66.160718
1440.000914	38.928415	66.165722
1438.763901	32.990954	66.170727
1438.021234	30.694796	66.175732
1437.414197	33.691177	66.180737
1436.934961	27.800435	66.185742
1436.834262	29.893212	66.190746
1435.536867	34.891572	66.195751
1434.999801	31.700183	66.200756
1434.104232	28.625694	66.205761
1433.949084	34.484836	66.210766
1432.905536	36.792114	66.215770
1431.897655	29.704962	66.220775
1431.727285	25.775658	66.225780
1431.145833	36.543584	66.230785
1430.292294	26.856854	66.235790
1429.577650	37.964479	66.240794
1428.738680	38.455789	66.245799
1428.663096	29.159479	66.250804
1427.939857	32.844506	66.255809
1427.133921	31.652764	66.260814
1426.304602	33.039787	66.265818
1425.689193	34.541040	66.270823
1425.228665	31.982434	66.275828
1424.373793	34.910980	66.280833
1423.397978	25.825558	66.285838
1423.090044	27.017756	66.290842
1422.048928	31.961198	66.295847
1421.977976	20.612634	66.300852
1421.101099	29.636172	66.305857
1420.244054	22.878277	66.310862
1419.932592	22.606114	66.315866
1419.047618	24.082405	66.320871
1418.950737	22.268638	66.325876
1417.761081	35.364518	66.330881
1417.188152	24.628721	66.335886
1416.839640	25.335382	66.340890
1415.356639	30.423172	66.345895
1414.728477	29.625783	66.350900
1413.995128	27.044313	66.355905
1413.488305	29.603743	66.360910
1413.533778	35.875680	66.365914
1412.933873	22.649545	66.370919
1412.106709	32.057828	66.375924
1410.831001	21.905223	66.380929
1410.204683	27.642140	66.385934
1410.185158	33.839255	66.390938
1409.284009	20.246283	66.395943
1408.526756	29.753836	66.400948
1407.914792	26.154909	66.405953
1407.445153	30.673225	66.410958
1406.381976	25.834049	66.415962
1405.525149	31.900906	66.420967
1405.329358	16.953245	66.425972
1404.762727	33.323050	66.430977
1403.996645	28.972793	66.435982
1403.172306	29.223676	66.440986
1402.449140	24.942290	66.445991
1402.201668	30.663147	66.450996
1401.354652	27.481610	66.456001
1400.566385	29.503907	66.461006
1400.196844	21.228842	66.466010
1399.401518	25.278553	66.471015
1398.949025	16.258196	66.476020
1397.657971	33.260361	66.481025
1397.201067	21.014402	66.486030
1396.675436	28.613383	66.491034
1396.287102	28.996809	66.496039
1395.239303	20.200376	66.501044
1394.258968	29.434321	66.506049
1394.034737	27.233961	66.511054
1393.799801	20.801377	66.516058
1392.799942	27.403456	66.521063
1391.915634	20.697214	66.526068
1391.022996	26.618384	66.531073
1390.671248	28.610722	66.536078
1390.182677	22.857089	66.541082
1389.039738	25.657975	66.546087
1388.789557	21.266722	66.551092
1387.796234	26.078004	66.556097
1387.486060	22.106277	66.561102
1387.094668	27.162489	66.566106
1385.968894	31.881290	66.571111
1385.935480	22.562519	66.576116
1384.829979	25.087809	66.581121
1383.932768	23.134763	66.586126
1383.117972	18.402770	66.591130
1382.393524	19.322149	66.596135
1382.393005	14.079122	66.601140
1381.741494	25.955689	66.606145
1380.846373	10.332337	66.611150
1380.224039	17.673885	66.616154
1379.461877	21.224766	66.621159
1379.031469	20.362838	66.626164
1377.882807	21.439530	66.631169
1377.068421	22.338515	66.636174
1376.553196	26.679585	66.641178
1376.272811	23.467911	66.646183
1376.177694	20.266211	66.651188
1374.924637	25.872532	66.656193
1374.822735	18.699747	66.661198
1373.859733	13.043612	66.666202
1372.444536	15.241259	66.671207
1372.201363	18.247619	66.676212
1371.332485	19.346069	66.681217
1371.060206	23.698982	66.686222
1370.256649	16.926301	66.691226
1369.576281	28.616656	66.696231
1368.882269	21.326689	66.701236
1368.333066	22.666049	66.706241
1368.086299	18.736284	66.711246
1366.772247	20.824821	66.716250
1366.134709	27.752497	66.721255
1365.599468	19.107983	66.726260
1365.094872	21.660759	66.731265
1364.073791	22.313496	66.736270
1363.492522	16.500494	66.741274
1362.742351	25.568554	66.746279
1362.697683	22.158572	66.751284
1361.045139	29.104098	66.756289
1360.635316	21.303779	66.761294
1360.181843	19.538815	66.766298
1359.116893	23.516284	66.771303
1359.328464	17.883168	66.776308
1358.842816	21.502057	66.781313
1357.956530	23.079497	66.786318
1356.952235	21.304326	66.791322
1356.266656	33.553731	66.796327
1356.240079	21.942668	66.801332
1354.611953	29.803638	66.806337
1354.054336	31.585866	66.811342
1353.668345	24.264285	66.816346
1353.220337	24.166792	66.821351
1352.890505	16.642332	66.826356
1351.632573	21.281231	66.831361
1350.743874	25.963935	66.836366
1350.891765	25.719680	66.841370
1349.760419	30.034123	66.846375
1349.184250	14.727494	66.851380
1348.512904	38.306102	66.856385
1348.107443	20.236441	66.861390
1346.637672	18.164702	66.866394
1345.952365	22.644771	66.871399
1345.844833	21.558067	66.876404
1345.091975	32.362707	66.881409
1344.724267	15.964853	66.886414
1343.781363	26.022298	66.891418
1343.028937	27.515389	66.896423
1342.673873	29.760561	66.901428
1342.025368	33.646607	66.906433
1341.298369	23.269628	66.911438
1340.399587	22.267708	66.916442
1339.901938	31.779736	66.921447
1339.432811	18.524959	66.926452
1338.234906	27.802966	66.931457
1337.334988	28.553142	66.936462
1336.838139	25.099930	66.941466
1336.482873	25.815560	66.946471
1336.442421	16.029584	66.951476
1335.406513	19.646068	66.956481
1334.624490	19.590640	66.961486
1334.134409	25.102494	66.966490
1333.365247	21.058668	66.971495
1332.564240	16.952100	66.976500
1331.653581	21.021739	66.981505
1331.268350	23.795231	66.986510
1330.960356	19.813706	66.991514
1329.876353	31.317511	66.996519
1329.540574	15.543763	67.001524
1328.863693	13.579366	67.006529
1327.931278	20.915028	67.011534
1327.364081	11.357867	67.016538
1326.445800	29.507102	67.021543
1325.959417	23.264305	67.026548
1325.512897	16.713990	67.031553
1324.512494	19.312477	67.036558
1323.458024	15.258822	67.041562
1322.888322	30.586798	67.046567
1322.977384	14.125800	67.051572
1322.218507	25.566879	67.056577
1321.971401	16.081827	67.061582
1321.158646	22.442880	67.066586
1320.046338	18.723257	67.071591
1319.286575	16.663234	67.076596
1318.433866	25.977829	67.081601
1317.682903	19.270919	67.086606
1317.512824	29.982914	67.091610
1316.773991	28.443087	67.096615
1316.465437	22.260328	67.101620
1315.056036	20.284661	67.106625
1314.708805	23.777478	67.111630
1314.343799	20.134587	67.116634
1313.353230	20.344120	67.121639
1312.551206	11.760962	67.126644
1311.849205	25.066332	67.131649
1311.720014	11.620339	67.136654
1311.337335	23.000033	67.141658
1310.216582	16.091731	67.146663
1309.335439	18.401618	67.151668
1308.827309	15.470579	67.156673
1308.315797	22.622643	67.161678
1307.441363	14.785824	67.166682
1306.616422	20.538565	67.171687
1306.575074	20.797456	67.176692
1305.413531	20.007626	67.181697
1304.389463	25.856679	67.186702
1304.139061	13.983183	67.191706
1303.317495	30.136487	67.196711
1303.303917	10.618474	67.201716
1302.267284	24.380726	67.206721
1301.581386	21.416451	67.211726
1300.920656	23.060547	67.216730
1300.375454	24.322018	67.221735
1299.759603	24.244912	67.226740
1298.839900	22.527276	67.231745
1298.326942	17.681098	67.236750
1297.869683	15.771676	67.241754
1296.633761	21.883059	67.246759
1295.964624	10.289019	67.251764
1295.406644	32.797816	67.256769
1294.990885	25.621323	67.261774
1294.715607	16.164409	67.266778
1293.554599	23.386621	67.271783
1293.046440	13.775931	67.276788
1292.404265	22.049431	67.281793
1291.703332	20.265479	67.286798
1290.830585	11.890684	67.291802
1290.257412	29.582953	67.296807
1290.118181	10.945897	67.301812
1288.768384	33.019215	67.306817
1287.769847	13.377114	67.311822
1287.249510	9.864577	67.316826
1286.614649	20.721418	67.321831
1286.771010	5.061829	67.326836
1286.197547	19.502611	67.331841
1285.615882	19.744910	67.336846
1285.380413	10.070371	67.341850
1283.581596	23.299401	67.346855
1282.674863	15.098737	67.351860
1282.128603	14.975879	67.356865
1281.738387	10.649486	67.361870
1281.393733	19.653085	67.366874
1280.287191	26.261122	67.371879
1279.708808	15.376443	67.376884
1278.970940	18.874603	67.381889
1278.723928	26.087116	67.386894
1277.924971	19.357891	67.391898
1276.955573	17.610320	67.396903
1276.637360	11.957362	67.401908
1276.011233	14.608318	67.406913
1275.177130	22.762533	67.411918
1274.619229	22.363998	67.416922
1274.046747	13.720706	67.421927
1273.195444	11.419799	67.426932
1272.021583	16.717115	67.431937
1271.498132	19.872118	67.436942
1271.298271	15.728338	67.441946
1270.541135	20.623524	67.446951
1270.199909	9.612841	67.451956
1269.099073	13.905114	67.456961
1268.314265	15.545292	67.461966
1268.215497	21.706109	67.466970
1267.167200	26.912507	67.471975
1266.778530	11.019464	67.476980
1265.804776	17.229517	67.481985
1265.379137	25.159527	67.486990
1264.681923	20.426227	67.491994
1263.532704	27.506236	67.496999
1263.562193	12.713598	67.502004
1262.843071	27.567038	67.507009
1262.038272	14.349893	67.512014
1261.198874	21.366447	67.517018
1260.268618	31.694706	67.522023
1260.285467	14.382646	67.527028
1259.134245	21.456665	67.532033
1258.251315	20.158954	67.537038
1257.976709	7.940832	67.542042
1257.119638	22.578093	67.547047
1257.141716	16.536733	67.552052
1255.957405	22.395511	67.557057
1255.120257	18.010879	67.562062
1254.825030	18.470980	67.567066
1254.103649	18.241938	67.572071
1253.504501	11.745872	67.577076
1252.519965	15.240682	67.582081
1251.831312	14.971746	67.587086
1251.711040	6.677590	67.592090
1250.356103	14.816854	67.597095
1249.674997	13.654206	67.602100
1249.202663	17.496487	67.607105
1248.881527	5.227423	67.612110
1248.438542	10.417996	67.617114
1247.200572	19.066920	67.622119
1246.748516	12.627888	67.627124
1246.056904	16.885063	67.632129
1245.528505	19.637176	67.637134
1244.875757	13.308899	67.642138
1243.925893	25.035812	67.647143
1243.831636	18.815839	67.652148
1242.883863	21.812823	67.657153
1242.204619	28.409700	67.662158
1241.772496	15.937514	67.667162
1240.667882	25.678515	67.672167
1239.710269	15.759278	67.677172
1239.065805	21.065467	67.682177
1238.480046	22.861654	67.687182
1238.492272	16.884936	67.692186
1238.006571	21.847352	67.697191
1237.401319	10.468670	67.702196
1236.443603	15.597597	67.707201
1235.363641	17.147528	67.712206
1234.286434	8.344822	67.717210
1233.445487	20.440750	67.722215
1233.362261	11.755945	67.727220
1233.001276	25.874382	67.732225
1232.584900	19.301950	67.737230
1232.223909	4.338037	67.742234
1231.146235	14.232438	67.747239
1230.761404	12.491277	67.752244
1229.448051	14.267547	67.757249
1228.576709	22.938604	67.762254
1228.226926	15.770563	67.767258
1227.453122	25.851609	67.772263
1227.168165	21.364990	67.777268
1226.165888	29.121781	67.782273
1225.552513	23.321807	67.787278
1225.148548	19.645706	67.792282
1224.109497	23.720026	67.797287
1223.380662	22.648549	67.802292
1223.005893	23.644825	67.807297
1222.634459	15.877861	67.812302
1221.774922	17.868964	67.817306
1220.554629	26.712202	67.822311
1220.086801	12.116917	67.827316
1219.969028	22.364867	67.832321
1219.327276	13.179123	67.837326
1218.541001	18.091570	67.842330
1217.518240	21.079987	67.847335
1217.072591	13.129294	67.852340
1216.586736	18.437072	67.857345
1215.374778	16.579870	67.862350
1214.709849	11.595463	67.867354
1214.110406	19.425384	67.872359
1214.153089	2.580725	67.877364
1213.285094	10.659917	67.882369
1212.314747	25.897069	67.887374
1211.689357	15.494529	67.892378
1211.226769	21.478243	67.897383
1210.296702	13.462664	67.902388
1209.522899	23.075379	67.907393
1208.760763	32.347216	67.912398
1208.758159	19.748390	67.917402
1208.006356	25.748136	67.922407
1207.357849	21.313024	67.927412
1206.542840	14.162202	67.932417
1206.104802	15.157503	67.937422
1204.937385	20.223598	67.942426
1204.248527	22.484019	67.947431
1203.700887	11.927202	67.952436
1203.196658	22.247643	67.957441
1202.765425	15.425281	67.962446
1201.974274	9.301947	67.967450
1201.024344	17.860931	67.972455
1200.682332	15.736091	67.977460
1199.901828	20.729623	67.982465
1199.298682	17.558265	67.987470
1198.918916	17.561906	67.992474
1197.799534	18.635597	67.997479
1196.716115	20.931957	68.002484
1196.079506	18.973809	68.007489
1195.759209	16.146961	68.012494
1195.652055	10.335882	68.017498
1195.183181	19.116399	68.022503
1194.417150	10.273689	68.027508
1193.669112	17.496493	68.032513
1192.397912	22.159649	68.037518
1191.764130	15.948214	68.042522
1190.764409	24.556122	68.047527
1190.972697	20.416827	68.052532
1190.209643	12.049862	68.057537
1188.903241	19.973290	68.062542
1188.454880	16.892431	68.067546
1187.940611	22.086467	68.072551
1187.630455	15.063514	68.077556
1186.468397	14.723231	68.082561
1185.693808	18.302944	68.087566
1185.353631	19.643790	68.092570
1184.907641	25.364685	68.097575
1183.932536	18.409632	68.102580
1183.070831	19.721458	68.107585
1182.465469	23.113419	68.112590
1182.314387	12.712730	68.117594
1181.645153	22.540622	68.122599
1180.675570	20.867231	68.127604
1180.082159	14.830721	68.132609
1179.703880	23.182115	68.137614
1178.966575	11.168474	68.142618
1177.807478	15.734963	68.147623
1177.347362	6.387895	68.152628
1177.001401	16.523900	68.157633
1175.969474	24.588181	68.162638
1175.603421	16.907100	68.167642
1175.021966	23.109986	68.172647
1174.179812	13.446797	68.177652
1172.958100	25.079772	68.182657
1172.569486	13.849576	68.187662
1172.060956	25.288711	68.192666
1171.457240	15.742137	68.197671
1170.811019	17.388687	68.202676
1169.788724	23.303731	68.207681
1169.111078	19.362097	68.212686
1168.988995	30.014415	68.217690
1168.328264	14.681884	68.222695
1167.524666	21.531927	68.227700
1166.904074	25.829864	68.232705
1166.408577	20.028508	68.237710
1165.794998	19.276170	68.242714
1164.594011	20.657730	68.247719
1164.255149	18.229635	68.252724
1163.721876	13.374108	68.257729
1163.041371	11.954358	68.262734
1162.287311	15.565503	68.267738
1161.408500	20.727636	68.272743
1160.755685	17.587840	68.277748
1160.121536	10.917605	68.282753
1159.293132	15.828882	68.287758
1158.611264	5.369121	68.292762
1158.053021	16.108139	68.297767
1157.722200	2.140770	68.302772
1157.393511	17.116612	68.307777
1156.414998	21.190790	68.312782
1156.067165	10.113381	68.317786
1155.036389	11.721750	68.322791
1154.523474	14.435148	68.327796
1153.851053	11.971800	68.332801
1152.667545	16.105386	68.337806
1151.721446	7.620901	68.342810
1151.196102	20.524471	68.347815
1150.897310	15.589080	68.352820
1150.342086	19.944428	68.357825
1150.072253	10.111386	68.362830
1149.437004	9.515456	68.367834
1148.308413	21.442693	68.372839
1147.839582	19.885208	68.377844
1147.129068	18.271548	68.382849
1145.830005	14.457138	68.387854
1145.309046	10.851699	68.392858
1145.091397	17.857700	68.397863
1145.017099	15.529450	68.402868
1143.811100	20.450326	68.407873
1142.744966	23.805197	68.412878
1142.535348	14.937087	68.417882
1141.783336	21.802584	68.422887
1140.796435	18.960345	68.427892
1139.726371	17.788630	68.432897
1139.467378	18.783849	68.437902
1139.782002	11.779804	68.442906
1138.718157	20.993983	68.447911
1138.022375	10.741433	68.452916
1137.171355	15.478126	68.457921
1136.617041	12.972345	68.462926
1135.774931	8.553859	68.467930
1134.832247	22.290169	68.472935
1134.548261	20.340606	68.477940
1134.224606	23.440202	68.482945
1133.120619	17.453374	68.487950
1132.559990	14.024549	68.492954
1131.707677	18.915983	68.497959
1131.410096	14.686843	68.502964
1130.224324	22.545382	68.507969
1129.360426	21.506453	68.512974
1129.189731	14.934393	68.517978
1128.635952	18.471117	68.522983
1128.040952	17.662219	68.527988
1127.027041	16.923104	68.532993
1126.228520	14.591778	68.537998
1126.232386	11.994066	68.543002
1125.429708	21.534122	68.548007
1124.544015	21.400634	68.553012
1123.767486	22.263715	68.558017
1123.213985	23.556502	68.563022
1122.916100	17.340547	68.568026
1121.626813	18.239454	68.573031
1121.043948	20.738491	68.578036
1120.407753	24.253634	68.583041
1120.393165	14.359499	68.588046
1119.637418	15.935177	68.593050
1118.318276	16.343695	68.598055
1118.034179	10.283238	68.603060
1117.379355	16.068890	68.608065
1116.620671	17.788532	68.613070
1116.088143	15.181524	68.618074
1115.663094	19.820510	68.623079
1114.783784	13.821610	68.628084
1113.936830	19.420214	68.633089
1113.495616	23.203953	68.638094
1113.079481	18.678296	68.643098
1111.881197	19.138554	68.648103
1111.316423	17.793446	68.653108
1110.660346	15.628693	68.658113
1109.972187	23.113215	68.663118
1109.163970	13.977641	68.668122
1108.334655	21.971870	68.673127
1108.024685	16.180443	68.678132
1107.776391	23.940338	68.683137
1106.618235	21.806562	68.688142
1105.890062	17.589147	68.693146
1105.129652	22.639429	68.698151
1104.908877	16.542093	68.703156
1104.442243	17.447346	68.708161
1103.299722	21.353673	68.713166
1102.597507	19.886933	68.718170
1101.948973	26.147807	68.723175
1101.728584	13.906903	68.728180
1100.697576	22.053057	68.733185
1099.886916	22.886883	68.738190
1099.899336	13.511977	68.743194
1098.639242	21.219931	68.748199
1097.853313	16.757829	68.753204
1097.341821	15.784276	68.758209
1096.931757	22.543356	68.763214
1096.576618	19.677912	68.768218
1095.428892	24.149592	68.773223
1094.708531	14.370876	68.778228
1094.237683	17.385083	68.783233
1093.481416	28.005812	68.788238
1092.763251	16.771288	68.793242
1092.151739	30.085949	68.798247
1091.763042	9.441843	68.803252
1091.390988	14.909721	68.808257
1090.007585	23.430462	68.813262
1089.794327	17.111170	68.818266
1088.898722	21.832893	68.823271
1088.639718	14.950050	68.828276
1087.346291	21.375004	68.833281
1086.407145	19.122827	68.838286
1086.214723	13.397858	68.843290
1085.688140	23.606754	68.848295
1084.784117	21.334798	68.853300
1083.965638	18.081035	68.858305
1083.703839	22.250956	68.863310
1083.434979	16.713178	68.868314
1082.097330	24.050296	68.873319
1081.624241	16.920823	68.878324
1081.226739	17.084991	68.883329
1080.577104	18.366271	68.888334
1079.698341	14.973873	68.893338
1078.789438	19.538450	68.898343
1078.514837	15.912760	68.903348
1077.545771	22.604651	68.908353
1076.668853	19.538373	68.913358
1076.189492	18.849858	68.918362
1075.776885	18.428255	68.923367
1075.301081	17.920515	68.928372
1074.562748	23.167555	68.933377
1073.598163	14.455819	68.938382
1073.382349	13.903569	68.943386
1072.606908	15.414587	68.948391
1071.836249	18.960591	68.953396
1071.382155	20.206037	68.958401
1070.572558	19.691474	68.963406
1069.363228	17.669931	68.968410
1068.686354	27.536903	68.973415
1068.327014	16.308386	68.978420
1067.842263	18.266726	68.983425
1067.353146	24.369790	68.988430
1066.496938	14.138055	68.993434
1066.042459	12.283428	68.998439
1065.296710	12.148199	69.003444
1064.409638	16.550042	69.008449
1063.470644	21.108373	69.013454
1063.353459	11.490751	69.018458
1062.586203	24.798647	69.023463
1062.062034	22.212398	69.028468
1061.048224	23.300891	69.033473
1060.564599	22.974162	69.038478
1060.095331	18.825958	69.043482
1058.878298	25.524188	69.048487
1058.322086	20.812678	69.053492
1057.908439	25.758926	69.058497
1057.192581	21.206847	69.063502
1056.217004	16.353904	69.068506
1055.611264	29.205625	69.073511
1055.258358	22.501717	69.078516
1054.741226	22.896220	69.083521
1053.984428	25.377211	69.088526
1053.485307	18.892098	69.093530
1052.796723	15.091006	69.098535
1051.861328	17.409606	69.103540
1050.985334	19.994709	69.108545
1050.254151	15.225886	69.113550
1050.147145	14.932282	69.118554
1049.285817	23.133458	69.123559
1048.936938	9.735083	69.128564
1047.948549	20.056866	69.133569
1047.146834	18.940268	69.138574
1046.897392	22.420708	69.143578
1045.496398	23.655953	69.148583
1044.855473	9.525063	69.153588
1044.273411	20.576952	69.158593
1043.949221	24.190703	69.163598
1043.940979	16.446424	69.168602
1042.995717	22.678822	69.173607
1042.139570	18.770355	69.178612
1041.528540	19.329602	69.183617
1040.656167	17.765376	69.188622
1039.835288	16.077847	69.193626
1039.218618	19.017495	69.198631
1038.978925	25.675365	69.203636
1038.239128	22.311333	69.208641
1036.957269	11.931296	69.213646
1036.878573	17.593773	69.218650
1036.470876	29.694936	69.223655
1035.572768	20.192085	69.228660
1035.011041	15.328504	69.233665
1034.289587	22.529769	69.238670
1033.020857	19.511647	69.243674
1032.268004	22.996485	69.248679
1031.994621	24.468643	69.253684
1031.517567	22.996063	69.258689
1031.072507	26.826154	69.263694
1030.470560	19.263054	69.268698
1029.696175	28.815979	69.273703
1029.085658	9.520723	69.278708
1028.028940	21.600559	69.283713
1027.645837	16.874134	69.288718
1027.166629	13.124892	69.293722
1025.798977	24.724368	69.298727
1025.324477	21.269252	69.303732
1024.524143	15.789230	69.308737
1023.923618	26.512920	69.313742
1023.973501	12.909191	69.318746
1022.901005	19.902967	69.323751
1022.173433	29.054228	69.328756
1021.709309	20.403235	69.333761
1020.926245	24.020609	69.338766
1019.885947	17.497030	69.343770
1019.212474	26.288040	69.348775
1018.755624	18.377023	69.353780
1018.550876	22.823286	69.358785
1017.475758	22.729433	69.363790
1016.876286	20.159905	69.368794
1016.030257	25.894002	69.373799
1015.544452	33.437813	69.378804
1015.246429	27.794301	69.383809
1014.063515	21.720745	69.388814
1013.810347	14.868524	69.393818
1012.983013	33.714514	69.398823
1012.335046	16.891448	69.403828
1011.256280	27.960871	69.408833
1010.795337	22.584544	69.413838
1010.872840	23.366976	69.418842
1009.864788	17.544711	69.423847
1009.242999	22.265471	69.428852
1008.658772	23.228872	69.433857
1007.412214	25.297387	69.438862
1006.431655	18.029485	69.443866
1005.667880	26.543143	69.448871
1005.336598	16.320955	69.453876
1005.217589	25.616657	69.458881
1004.818567	32.129577	69.463886
1004.188847	24.799547	69.468890
1003.150519	20.429672	69.473895
1002.681739	20.788109	69.478900
1001.389155	29.639779	69.483905
1000.796698	26.438388	69.488910
1000.679825	21.379465	69.493914
1000.108726	22.900570	69.498919
998.757254	27.699582	69.503924
998.193218	21.620605	69.508929
997.375955	35.854219	69.513934
997.661928	24.188746	69.518938
996.176184	26.681656	69.523943
995.496946	20.901693	69.528948
995.146317	23.966172	69.533953
994.968575	22.152680	69.538958
994.036368	15.298118	69.543962
992.990643	22.871090	69.548967
992.213636	22.504324	69.553972
991.756484	20.751056	69.558977
991.213225	26.493756	69.563982
990.489929	12.117384	69.568986
989.918907	25.945976	69.573991
989.477828	8.501839	69.578996
988.812137	18.706066	69.584001
987.658519	23.590290	69.589006
987.439693	26.573879	69.594010
986.807432	25.070812	69.599015
985.607822	23.044610	69.604020
984.768301	23.536151	69.609025
984.341377	24.217499	69.614030
984.316959	12.566730	69.619034
983.017630	25.104630	69.624039
982.287374	19.487324	69.629044
981.874299	22.060294	69.634049
981.487355	23.351839	69.639054
980.624507	11.648401	69.644058
979.976585	19.093429	69.649063
979.718728	12.029084	69.654068
979.068434	11.951228	69.659073
977.734285	21.713065	69.664078
977.202491	14.493619	69.669082
976.510733	14.236290	69.674087
976.423629	12.299576	69.679092
975.155185	14.609694	69.684097
974.530112	20.838473	69.689102
974.288751	13.511320	69.694106
972.871350	19.732133	69.699111
972.552144	17.288326	69.704116
971.912279	15.671362	69.709121
971.566809	11.009921	69.714126
970.877240	11.804020	69.719130
969.755783	10.203763	69.724135
969.457339	23.886488	69.729140
968.923452	22.359889	69.734145
967.863682	15.670708	69.739150
967.165784	10.578091	69.744154
966.234891	21.792720	69.749159
966.192209	14.962207	69.754164
965.690622	11.470418	69.759169
964.381901	23.678675	69.764174
963.793269	13.691403	69.769178
963.221420	13.495420	69.774183
963.084141	10.366689	69.779188
962.392847	26.813107	69.784193
961.320337	22.205851	69.789198
961.095770	14.182202	69.794202
960.377224	16.950429	69.799207
959.195364	10.006305	69.804212
958.576846	11.974910	69.809217
957.974665	20.084412	69.814222
958.035454	5.988556	69.819226
956.555561	15.718397	69.824231
956.028871	18.191183	69.829236
955.683780	13.635335	69.834241
954.793727	10.659500	69.839246
953.909665	13.441449	69.844250
953.256262	17.645304	69.849255
952.908318	8.774012	69.854260
952.739930	15.729599	69.859265
951.467117	20.672226	69.864270
950.914449	9.406702	69.869274
949.967666	19.537397	69.874279
950.020896	16.890837	69.879284
948.486277	18.243585	69.884289
948.114087	15.240539	69.889294
947.848397	13.959838	69.894298
946.920261	18.109644	69.899303
946.030812	20.482467	69.904308
945.608570	11.783838	69.909313
945.381167	17.980881	69.914318
944.573659	13.586921	69.919322
943.366728	23.837860	69.924327
943.079133	14.990078	69.929332
942.545271	18.525242	69.934337
941.418933	17.881359	69.939342
940.841559	14.463132	69.944346
940.303433	20.764810	69.949351
940.007189	13.913150	69.954356
939.011177	11.034602	69.959361
937.877805	16.150577	69.964366
937.631110	14.535711	69.969370
937.222140	16.652316	69.974375
936.209846	18.707239	69.979380
935.375892	9.992131	69.984385
934.863184	24.759147	69.989390
934.682468	18.308551	69.994394
933.398227	11.172585	69.999399
932.983317	5.014715	70.004404
932.406546	19.266821	70.009409
931.665255	12.254182	70.014414
931.461164	11.577084	70.019418
929.958693	18.894765	70.024423
929.564368	3.799064	70.029428
929.294642	18.571560	70.034433
928.653324	19.466797	70.039438
927.586267	14.415590	70.044442
927.062141	18.113202	70.049447
926.645859	17.769476	70.054452
925.691658	23.336315	70.059457
925.072875	17.289727	70.064462
924.640440	19.195615	70.069466
923.861370	12.665206	70.074471
923.209305	17.529563	70.079476
922.523069	14.880833	70.084481
922.144174	28.320909	70.089486
921.155911	17.605652	70.094490
920.330549	29.364872	70.099495
919.525534	17.715330	70.104500
919.328761	18.331680	70.109505
918.263510	24.242607	70.114510
917.190816	20.444337	70.119514
916.736811	20.483487	70.124519
916.644675	26.846656	70.129524
916.626252	12.930553	70.134529
915.486170	26.026580	70.139534
914.878634	24.008691	70.144538
914.136806	20.425839	70.149543
912.654139	23.965348	70.154548
912.125517	18.506781	70.159553
911.423585	19.961996	70.164558
911.286393	15.548105	70.169562
910.599818	15.974332	70.174567
910.491160	23.910694	70.179572
909.352646	14.946031	70.184577
908.479878	18.356947	70.189582
908.686558	19.098318	70.194586
907.170092	19.593538	70.199591
906.648199	11.382263	70.204596
906.231842	24.833028	70.209601
905.304899	21.429440	70.214606
904.953299	12.112484	70.219610
904.279636	20.195525	70.224615
903.359924	21.914045	70.229620
902.739146	17.810488	70.234625
901.897017	20.560552	70.239630
901.559634	16.888112	70.244634
900.305265	19.312716	70.249639
899.220117	12.369002	70.254644
899.007944	17.836684	70.259649
898.801913	16.469228	70.264654
898.553218	19.227350	70.269658
897.396883	25.067628	70.274663
896.485241	15.863451	70.279668
896.227766	8.464765	70.284673
895.509833	24.409250	70.289678
894.692504	14.352746	70.294682
893.929144	27.507094	70.299687
893.547760	12.727864	70.304692
892.977997	20.316579	70.309697
891.905021	20.955685	70.314702
891.861755	2.699267	70.319706
890.873630	10.636817	70.324711
889.909643	11.651219	70.329716
888.986449	16.322201	70.334721
888.458197	9.209447	70.339726
888.572736	17.370467	70.344730
887.699263	18.348389	70.349735
886.712502	14.385079	70.354740
885.963252	4.994229	70.359745
885.698608	27.013221	70.364750
884.913275	-0.559521	70.369754
883.883571	13.647978	70.374759
883.602439	7.553978	70.379764
883.330264	16.292178	70.384769
881.929834	9.351345	70.389774
881.323984	6.242004	70.394778
880.818701	11.299039	70.399783
880.242945	0.882424	70.404788
879.320649	15.405551	70.409793
878.639683	5.111327	70.414798
878.252192	10.764596	70.419802
877.936324	5.453524	70.424807
877.140795	9.452942	70.429812
876.541556	17.353840	70.434817
875.571442	11.754248	70.439822
874.606596	15.471549	70.444826
873.356091	11.184387	70.449831
872.988059	19.482128	70.454836
873.051931	15.485650	70.459841
872.211678	14.438318	70.464846
872.061827	14.447992	70.469850
870.905587	13.077232	70.474855
870.429929	15.289612	70.479860
869.951164	6.158478	70.484865
869.239162	10.855774	70.489870
868.361244	6.408399	70.494874
867.718640	13.393728	70.499879
867.208025	13.024026	70.504884
866.106625	10.118130	70.509889
865.195162	15.782258	70.514894
865.097640	11.836697	70.519898
864.741072	10.207789	70.524903
863.993290	4.951269	70.529908
863.332634	12.155502	70.534913
862.515143	21.161835	70.539918
861.657462	13.283120	70.544922
860.675284	21.186625	70.549927
860.091511	2.059078	70.554932
860.203396	11.734309	70.559937
859.188285	13.989971	70.564942
858.396414	3.972014	70.569946
857.796810	13.784136	70.574951
857.201785	9.255472	70.579956
856.040729	-1.911604	70.584961
855.470262	8.217559	70.589966
855.388993	11.757970	70.594970
854.505208	12.633470	70.599975
853.254805	13.414365	70.604980
852.632116	15.025707	70.609985
852.345379	11.351524	70.614990
852.339870	13.692494	70.619994
851.578724	10.270427	70.624999
850.637827	7.589716	70.630004
850.328104	6.648754	70.635009
849.042366	9.172985	70.640014
848.319336	3.582966	70.645018
847.493058	14.929194	70.650023
847.392829	10.167247	70.655028
846.706106	5.137545	70.660033
845.664760	12.728785	70.665038
845.136662	4.406562	70.670042
845.071798	10.260783	70.675047
843.891935	11.700624	70.680052
843.030455	15.931313	70.685057
842.347583	19.914390	70.690062
842.226900	9.113130	70.695066
840.985515	9.980900	70.700071
840.454664	5.858321	70.705076
839.837180	7.079351	70.710081
839.544720	9.648909	70.715086
838.492255	13.184636	70.720090
837.792566	14.289447	70.725095
836.943058	12.784732	70.730100
836.847417	10.958187	70.735105
835.960523	11.790037	70.740110
835.313815	10.412307	70.745114
834.528315	9.471385	70.750119
834.384182	7.053349	70.755124
833.379739	11.956464	70.760129
832.129902	10.941224	70.765134
831.899581	11.968176	70.770138
831.334144	15.863180	70.775143
830.831089	1.778247	70.780148
829.786096	6.440248	70.785153
829.131662	14.343628	70.790158
829.008502	4.845263	70.795162
827.990504	9.362627	70.800167
827.422291	5.143502	70.805172
826.887173	5.099391	70.810177
826.253189	4.258928	70.815182
825.362824	1.814599	70.820186
824.321667	11.837348	70.825191
823.813116	7.354850	70.830196
823.515694	3.915751	70.835201
822.676248	18.159214	70.840206
822.050534	6.053854	70.845210
821.011372	20.497834	70.850215
820.696743	18.453847	70.855220
820.776689	3.643794	70.860225
819.184585	9.146627	70.865230
818.742927	-0.383034	70.870234
818.110023	10.776307	70.875239
817.680621	20.944527	70.880244
816.951529	6.282171	70.885249
816.193348	9.780524	70.890254
815.851523	6.993433	70.895258
814.840770	14.259710	70.900263
814.013090	14.460855	70.905268
813.521623	10.071829	70.910273
812.691483	15.246813	70.915278
811.776096	12.588862	70.920282
810.936231	15.234519	70.925287
810.611703	9.710382	70.930292
810.402299	9.956609	70.935297
809.709450	10.792271	70.940302
809.133845	11.719652	70.945306
808.505937	7.970479	70.950311
807.757629	11.391574	70.955316
806.697068	9.056340	70.960321
805.587205	12.318955	70.965326
805.236456	10.752206	70.970330
804.975047	13.285287	70.975335
804.539889	7.554847	70.980340
803.706379	10.513290	70.985345
803.152323	12.153141	70.990350
802.762350	9.551902	70.995354
801.511484	15.462452	71.000359
800.737886	15.298620	71.005364
800.304388	9.542685	71.010369
799.343080	7.477068	71.015374
798.551113	0.609739	71.020378
797.703078	16.992806	71.025383
797.272229	8.472198	71.030388
797.165023	8.169177	71.035393
796.525531	12.183202	71.040398
796.284732	6.962691	71.045402
795.099563	10.918506	71.050407
794.717725	14.536722	71.055412
793.691683	15.590998	71.060417
792.872529	12.942966	71.065422
792.294328	-0.598583	71.070426
791.682859	11.588621	71.075431
791.013926	8.419964	71.080436
790.267360	5.646845	71.085441
789.701682	17.574467	71.090446
789.639915	11.369874	71.095450
788.046531	13.198825	71.100455
787.422377	11.316074	71.105460
787.218235	4.877118	71.110465
786.533199	12.566191	71.115470
785.900232	6.771055	71.120474
785.153266	20.689162	71.125479
784.480809	11.801761	71.130484
784.254862	11.260612	71.135489
783.146857	19.390738	71.140494
782.623326	4.523798	71.145498
781.660311	16.342791	71.150503
780.752525	12.360649	71.155508
780.164064	7.042529	71.160513
779.421619	11.689501	71.165518
779.628225	6.072938	71.170522
778.580821	14.988158	71.175527
777.854417	15.086465	71.180532
777.443201	15.167712	71.185537
776.599305	20.543583	71.190542
775.687279	18.101142	71.195546
774.917337	13.857374	71.200551
774.324868	8.479971	71.205556
774.135543	11.704864	71.210561
773.278834	14.315369	71.215566
772.485111	14.042791	71.220570
771.989474	8.799777	71.225575
771.125613	16.097875	71.230580
770.441234	13.043640	71.235585
769.646486	13.114984	71.240590
769.341128	10.779387	71.245594
768.980012	13.957515	71.250599
767.985275	14.762403	71.255604
767.311254	14.546461	71.260609
766.380039	15.363314	71.265614
766.273577	0.396875	71.270618
764.902390	5.285859	71.275623
764.191939	6.001340	71.280628
764.079887	5.677015	71.285633
763.344539	5.874516	71.290638
762.624626	6.134211	71.295642
761.631974	14.955570	71.300647
761.719372	3.613451	71.305652
761.155780	10.092659	71.310657
759.682678	14.018637	71.315662
759.339806	9.334748	71.320666
758.683549	6.944633	71.325671
758.135501	18.267088	71.330676
757.323431	5.215339	71.335681
756.328378	18.966374	71.340686
756.068402	9.603333	71.345690
755.526038	20.965883	71.350695
754.435049	14.775339	71.355700
754.000107	8.967609	71.360705
753.316803	13.051693	71.365710
753.215502	0.153288	71.370714
751.811838	12.504458	71.375719
751.254974	13.786817	71.380724
751.174868	4.554409	71.385729
749.997493	12.105838	71.390734
749.517221	8.382062	71.395738
748.557368	10.832385	71.400743
748.459322	10.278762	71.405748
747.254996	-1.748640	71.410753
746.546136	11.501114	71.415758
746.374918	4.620131	71.420762
745.613362	8.898013	71.425767
744.671601	12.351499	71.430772
744.096978	1.110048	71.435777
743.381527	10.801862	71.440782
742.961659	-0.520993	71.445786
741.975372	6.277810	71.450791
741.140427	8.295110	71.455796
740.974199	12.369413	71.460801
740.439684	13.164117	71.465806
740.178445	10.695351	71.470810
739.102250	14.353158	71.475815
738.299441	13.350371	71.480820
737.394044	16.061674	71.485825
736.017711	18.089479	71.490830
735.630982	10.867509	71.495834
735.389077	22.294186	71.500839
735.067609	12.412686	71.505844
734.823340	18.787451	71.510849
733.524465	16.980595	71.515854
733.157491	3.274556	71.520858
732.302342	16.252732	71.525863
731.244716	12.840062	71.530868
730.756776	12.201864	71.535873
730.199945	12.333109	71.540878
729.960594	11.269002	71.545882
729.072853	9.516536	71.550887
727.831713	16.527801	71.555892
727.787557	8.355633	71.560897
727.286284	13.137678	71.565902
726.326000	6.612545	71.570906
725.234915	16.963380	71.575911
725.075290	15.995384	71.580916
724.470354	10.107498	71.585921
723.323390	12.636503	71.590926
723.014164	6.453971	71.595930
722.399153	15.844388	71.600935
722.112741	8.399882	71.605940
721.177474	12.131448	71.610945
720.496227	8.417599	71.615950
719.982028	1.990175	71.620954
718.847770	17.395438	71.625959
717.982082	15.642618	71.630964
717.822731	10.571568	71.635969
717.051632	19.685658	71.640974
716.617198	7.125706	71.645978
715.403728	8.154663	71.650983
714.817410	11.124237	71.655988
714.932137	12.600859	71.660993
713.344893	10.168182	71.665998
712.694443	10.419985	71.671002
711.988712	6.869302	71.676007
712.009271	9.187195	71.681012
711.769639	-1.268684	71.686017
710.603140	6.358292	71.691022
709.771769	-1.675917	71.696026
709.332802	0.068623	71.701031
708.326640	11.452978	71.706036
707.746865	8.255959	71.711041
706.980211	8.255045	71.716046
706.826083	7.623626	71.721050
705.762251	12.686043	71.726055
704.813847	14.294089	71.731060
704.624712	3.811245	71.736065
703.795539	12.236027	71.741070
703.712253	11.568098	71.746074
702.679578	6.456337	71.751079
701.973892	9.083816	71.756084
701.167702	-0.025092	71.761089
699.954728	10.329385	71.766094
699.941969	11.331168	71.771098
699.474587	5.615345	71.776103
699.015555	10.680811	71.781108
698.022687	2.039995	71.786113
697.487430	19.016641	71.791118
696.837381	11.377738	71.796122
695.944659	19.971908	71.801127
694.945213	13.932389	71.806132
694.561417	8.614820	71.811137
693.781505	16.484591	71.816142
693.286483	7.053338	71.821146
692.187603	13.587828	71.826151
691.662448	12.827838	71.831156
691.692431	4.560297	71.836161
690.690490	17.147139	71.841166
689.930981	-3.396754	71.846170
689.446068	10.104338	71.851175
688.705669	7.475342	71.856180
687.864049	0.379432	71.861185
687.047601	11.873928	71.866190
686.783519	0.307100	71.871194
686.372429	12.951240	71.876199
685.176151	10.541481	71.881204
684.479641	12.968818	71.886209
683.977916	10.047945	71.891214
683.672410	11.930503	71.896218
682.380068	10.840111	71.901223
681.624598	12.609822	71.906228
681.168397	8.546356	71.911233
680.769459	11.435642	71.916238
680.718183	6.678531	71.921242
679.545684	17.638401	71.926247
678.412059	3.005833	71.931252
678.680983	1.379856	71.936257
677.417939	15.156233	71.941262
676.932741	-4.135145	71.946266
676.134790	10.259416	71.951271
674.832318	6.132018	71.956276
674.459097	-7.721224	71.961281
673.871688	10.734932	71.966286
673.503192	3.289316	71.971290
672.927052	3.444147	71.976295
672.306502	3.077800	71.981300
671.452053	11.877177	71.986305
670.998583	3.729195	71.991310
670.438266	2.120147	71.996314
669.369883	4.649277	72.001319
668.664723	10.444606	72.006324
668.226176	0.659038	72.011329
667.600183	14.737657	72.016334
667.241828	3.048656	72.021338
666.175069	14.253449	72.026343
665.742392	4.217801	72.031348
664.853947	11.575030	72.036353
663.616443	13.974983	72.041358
663.445484	11.797763	72.046362
662.947349	9.719947	72.051367
662.577816	6.357006	72.056372
661.570128	8.252035	72.061377
660.519287	10.201242	72.066382
660.566374	5.598773	72.071386
659.765563	-3.883112	72.076391
659.082590	10.288150	72.081396
658.398443	7.751126	72.086401
657.497523	14.356603	72.091406
656.764791	11.475674	72.096410
656.276863	13.696349	72.101415
655.486784	15.115208	72.106420
655.641988	8.196449	72.111425
654.086831	7.523216	72.116430
653.491234	4.000744	72.121434
652.628796	4.128633	72.126439
652.300256	11.432975	72.131444
652.006038	2.485398	72.136449
650.445670	8.539908	72.141454
650.430193	8.734767	72.146458
649.966859	3.313187	72.151463
649.015828	-1.595515	72.156468
648.359708	5.256391	72.161473
647.637093	5.612738	72.166478
647.375088	7.045273	72.171482
646.385682	9.766829	72.176487
645.725603	9.075641	72.181492
644.980947	4.635518	72.186497
644.386736	10.168770	72.191502
643.991502	-1.019213	72.196506
642.907134	12.490614	72.201511
642.711154	5.120029	72.206516
642.096185	7.603774	72.211521
640.796094	15.165327	72.216526
640.313715	16.462656	72.221530
639.641670	5.594701	72.226535
639.216339	9.215129	72.231540
638.337420	6.102034	72.236545
637.265774	15.196192	72.241550
637.096662	6.574027	72.246554
636.840206	3.328695	72.251559
636.130388	9.042775	72.256564
635.495724	0.736011	72.261569
634.638036	6.169303	72.266574
633.811724	7.212336	72.271578
633.116797	6.413166	72.276583
632.660546	10.073210	72.281588
632.298875	3.553715	72.286593
630.546610	14.747842	72.291598
630.150818	6.934441	72.296602
629.680050	4.254642	72.301607
629.147038	0.979240	72.306612
629.017723	-2.598555	72.311617
627.657960	5.589056	72.316622
627.134783	2.215899	72.321626
626.632887	4.809367	72.326631
625.700192	1.952409	72.331636
625.117428	5.061775	72.336641
624.364580	14.439464	72.341646
624.113554	6.702353	72.346650
623.697388	11.300558	72.351655
622.675503	4.337454	72.356660
622.177801	1.833825	72.361665
621.140461	7.212157	72.366670
620.249606	1.412415	72.371674
619.250489	9.291877	72.376679
618.859550	6.501602	72.381684
618.841469	0.786785	72.386689
618.406371	4.514420	72.391694
617.991095	2.860211	72.396698
617.147020	6.323412	72.401703
616.342253	4.466317	72.406708
615.323135	4.488291	72.411713
614.801139	8.024774	72.416718
614.233363	8.214554	72.421722
612.903404	8.445295	72.426727
612.069787	5.969934	72.431732
612.189527	7.111455	72.436737
611.590997	18.175473	72.441742
610.821417	2.491545	72.446746
609.801010	4.528960	72.451751
609.159904	3.710188	72.456756
608.961477	2.589118	72.461761
608.243430	12.368098	72.466766
607.285081	-1.951732	72.471770
606.489069	5.198412	72.476775
606.083902	15.395895	72.481780
606.059297	13.406672	72.486785
604.621770	10.374667	72.491790
603.869985	15.852603	72.496794
603.655093	2.718438	72.501799
603.016811	5.059256	72.506804
602.169079	-3.046414	72.511809
601.541615	3.864011	72.516814
601.186093	2.944569	72.521818
599.756537	-0.993820	72.526823
599.114065	7.722931	72.531828
599.105569	10.904839	72.536833
598.408553	19.705973	72.541838
597.315172	3.064426	72.546842
596.802123	0.545902	72.551847
595.863690	3.002328	72.556852
595.907690	0.581158	72.561857
594.614459	7.052021	72.566862
594.208453	7.484109	72.571866
593.845808	5.064627	72.576871
593.079697	1.533061	72.581876
592.131406	-4.446743	72.586881
591.014657	4.539496	72.591886
590.843172	5.765242	72.596890
590.310686	5.624573	72.601895
589.791590	7.380317	72.606900
588.731167	-3.640210	72.611905
588.080521	11.380573	72.616910
587.818321	9.590032	72.621914
586.845335	2.885648	72.626919
585.917356	10.555107	72.631924
585.809941	2.200655	72.636929
585.373422	9.474891	72.641934
584.806982	6.599039	72.646938
583.645882	12.642035	72.651943
583.034579	9.983051	72.656948
582.102606	-4.594838	72.661953
581.215528	6.456786	72.666958
580.708427	6.108661	72.671962
580.389196	8.198408	72.676967
579.742123	9.241294	72.681972
578.979031	4.953933	72.686977
578.386702	16.702902	72.691982
578.224341	9.057327	72.696986
577.074196	3.518083	72.701991
576.054795	-1.737647	72.706996
575.730857	0.106859	72.712001
575.396061	6.082902	72.717006
574.545560	1.208679	72.722010
573.807628	-1.728159	72.727015
573.083030	3.475806	72.732020
572.729788	4.145485	72.737025
571.542229	9.781137	72.742030
570.770459	2.697802	72.747034
570.580753	6.930379	72.752039
569.903167	3.763168	72.757044
569.137653	5.696928	72.762049
568.255263	6.078745	72.767054
567.908578	5.457505	72.772058
566.856391	8.096054	72.777063
566.146072	1.576913	72.782068
565.842045	6.554633	72.787073
565.122194	12.022760	72.792078
564.818223	2.135367	72.797082
564.011982	4.220686	72.802087
563.068981	2.860263	72.807092
562.741685	-0.015827	72.812097
561.576504	10.037792	72.817102
560.771530	-0.854684	72.822106
560.021757	5.643169	72.827111
559.660356	3.944122	72.832116
559.702341	3.325629	72.837121
558.506918	18.587725	72.842126
557.817284	9.130742	72.847130
557.381640	15.217465	72.852135
556.504041	10.921541	72.857140
555.992697	-0.101275	72.862145
554.870820	7.255318	72.867150
554.634686	4.257482	72.872154
554.326847	1.498136	72.877159
553.241707	6.185555	72.882164
552.573325	1.525170	72.887169
551.786825	16.928703	72.892174
551.573345	11.643957	72.897178
550.531782	3.307419	72.902183
549.870575	1.347061	72.907188
549.578837	-3.616149	72.912193
548.207427	9.888963	72.917198
547.647796	-4.295655	72.922202
547.195129	5.459984	72.927207
546.736264	6.132298	72.932212
546.383344	1.492628	72.937217
544.958682	11.970762	72.942222
544.399876	1.483758	72.947226
544.246112	4.281971	72.952231
543.636567	9.087595	72.957236
542.904819	-0.495124	72.962241
541.730010	3.467031	72.967246
541.545388	1.288846	72.972250
540.843125	4.942359	72.977255
539.604978	2.663916	72.982260
539.223115	3.722912	72.987265
538.698500	7.982029	72.992270
538.374760	2.273328	72.997274
537.585316	0.090563	73.002279
536.705378	3.233090	73.007284
536.537182	-10.272741	73.012289
535.149965	1.519260	73.017294
534.613667	0.101951	73.022298
533.996662	5.192599	73.027303
533.487154	2.604143	73.032308
533.175275	3.577881	73.037313
532.130060	8.385098	73.042318
531.885900	-3.328358	73.047322
530.646477	0.147381	73.052327
529.675759	5.422098	73.057332
529.580334	-8.711878	73.062337
529.003154	6.276704	73.067342
528.783528	-3.187320	73.072346
527.503695	6.135561	73.077351
526.864759	2.627912	73.082356
526.159713	-9.090967	73.087361
525.034365	0.208880	73.092366
524.607084	1.175771	73.097370
523.982714	-2.211200	73.102375
523.710691	2.450780	73.107380
523.468439	-1.044364	73.112385
522.141299	12.296022	73.117390
521.807881	1.607552	73.122394
520.751888	5.635942	73.127399
520.117823	3.418971	73.132404
519.258291	-6.939696	73.137409
518.590533	2.493834	73.142414
518.571665	-4.466570	73.147418
517.759752	5.404639	73.152423
516.976517	6.316275	73.157428
516.844601	-0.542549	73.162433
515.647951	7.303758	73.167438
514.820235	-0.726220	73.172442
514.140815	3.011964	73.177447
513.824133	-0.983804	73.182452
513.187241	2.364428	73.187457
512.125553	10.200278	73.192462
511.820497	-0.320828	73.197466
510.842281	1.744595	73.202471
509.823869	9.307062	73.207476
509.610230	-1.791545	73.212481
508.774249	2.760011	73.217486
508.589601	0.692215	73.222490
507.756489	-0.326167	73.227495
506.700967	9.315788	73.232500
506.288608	0.076421	73.237505
505.642248	9.203791	73.242510
505.336423	-1.359765	73.247514
504.386929	2.821967	73.252519
503.765034	5.680561	73.257524
503.336230	-5.719637	73.262529
502.305071	2.772054	73.267534
501.794086	3.839010	73.272538
500.918574	-0.597561	73.277543
500.501938	10.215150	73.282548
499.382978	0.312529	73.287553
498.773767	6.152530	73.292558
498.525942	-1.143541	73.297562
498.080247	6.919018	73.302567
496.905846	4.704555	73.307572
496.409392	5.950536	73.312577
495.554149	-3.286078	73.317582
495.741052	-0.633591	73.322586
494.514469	2.367061	73.327591
493.563678	-3.683260	73.332596
493.415861	-6.113292	73.337601
492.743208	2.311830	73.342606
491.772903	-3.702267	73.347610
491.356479	1.906760	73.352615
490.570426	2.397830	73.357620
489.518790	1.431612	73.362625
489.167431	0.815859	73.367630
488.679546	2.665993	73.372634
488.147190	-1.976618	73.377639
486.565571	1.003331	73.382644
486.324294	-2.635459	73.387649
485.779591	4.055234	73.392654
485.324752	0.179245	73.397658
484.882454	1.929082	73.402663
483.783508	2.533074	73.407668
483.440249	3.210635	73.412673
482.995562	3.664672	73.417678
481.714153	3.728485	73.422682
480.919239	-3.199745	73.427687
480.611626	2.578019	73.432692
480.383625	-6.384795	73.437697
478.863665	3.037856	73.442702
478.124834	-0.192104	73.447706
477.961985	9.097927	73.452711
477.184199	-0.354437	73.457716
477.368233	-6.938753	73.462721
475.970917	0.155834	73.467726
475.417753	-3.661912	73.472730
474.912850	1.888676	73.477735
473.575922	-1.220770	73.482740
473.523311	-3.825231	73.487745
472.594079	0.777458	73.492750
472.240585	-3.923603	73.497754
471.315158	2.315264	73.502759
470.415948	2.080089	73.507764
470.479182	2.464248	73.512769
469.255550	5.040267	73.517774
468.409447	0.688904	73.522778
467.743985	-1.589278	73.527783
467.497134	3.268958	73.532788
467.087338	-4.742427	73.537793
465.878487	7.492674	73.542798
465.175248	-0.312701	73.547802
465.052352	-3.522518	73.552807
463.961590	8.320055	73.557812
463.092018	1.416339	73.562817
462.356505	4.370310	73.567822
462.347488	0.965741	73.572826
461.956673	-1.312043	73.577831
460.869619	1.257989	73.582836
460.916107	-4.998503	73.587841
459.426302	5.849568	73.592846
458.477547	-1.670698	73.597850
457.963931	-3.749154	73.602855
457.260353	2.563177	73.607860
457.390252	-4.513958	73.612865
456.006250	3.650785	73.617870
455.693068	-7.898698	73.622874
454.836200	-0.730941	73.627879
453.916976	-1.246757	73.632884
453.198630	-3.300479	73.637889
452.312638	8.627739	73.642894
452.279939	0.485318	73.647898
452.109593	-0.976083	73.652903
451.365435	2.859157	73.657908
450.563311	-1.483436	73.662913
449.329514	9.386931	73.667918
448.577743	7.548257	73.672922
448.117378	2.391166	73.677927
447.317301	8.517038	73.682932
447.432190	2.011539	73.687937
446.230161	2.948920	73.692942
445.402677	1.382493	73.697946
445.001933	6.839226	73.702951
444.333795	5.100764	73.707956
443.358752	-6.737484	73.712961
442.539915	8.161881	73.717966
442.311432	-4.892807	73.722970
442.122011	1.643521	73.727975
440.809658	9.803166	73.732980
440.456435	-3.794589	73.737985
439.615703	9.842047	73.742990
439.380761	0.429361	73.747994
438.220575	-7.766795	73.752999
437.458625	-5.163401	73.758004
437.319895	-4.035900	73.763009
435.955529	6.694432	73.768014
435.177825	-0.045723	73.773018
434.792962	-1.372025	73.778023
434.069690	7.887451	73.783028
433.858938	-6.163482	73.788033
433.423025	4.633377	73.793038
432.541019	0.874341	73.798042
431.945371	2.626543	73.803047
431.234679	3.925593	73.808052
430.355185	-6.078212	73.813057
429.377640	-1.660189	73.818062
429.088724	-3.110581	73.823066
428.701310	-3.007839	73.828071
427.614018	-0.896622	73.833076
427.075619	-0.932241	73.838081
426.512302	6.021609	73.843086
425.808425	4.422879	73.848090
425.134163	3.494328	73.853095
423.773488	1.437306	73.858100
423.795282	-0.649183	73.863105
423.272033	3.456778	73.868110
422.921451	-1.761948	73.873114
421.939440	-2.802304	73.878119
421.107373	4.035103	73.883124
420.504107	-1.051905	73.888129
419.343124	2.058172	73.893134
418.883860	-7.072774	73.898138
418.850520	-0.693772	73.903143
417.912658	-7.048874	73.908148
417.552714	3.168210	73.913153
416.587792	-0.320578	73.918158
416.172522	2.664376	73.923162
415.060598	-3.279816	73.928167
414.139035	7.550275	73.933172
413.762745	-1.751580	73.938177
413.342491	2.645460	73.943182
412.507441	3.010328	73.948186
411.684766	1.859438	73.953191
410.741066	-0.495813	73.958196
410.948071	-13.716063	73.963201
410.229054	2.827831	73.968206
409.492267	4.463762	73.973210
408.811378	5.089481	73.978215
408.010362	6.841297	73.983220
407.176595	-2.070714	73.988225
406.225496	4.372525	73.993230
406.200265	2.162650	73.998234
405.551075	-0.917576	74.003239
404.282619	-0.888900	74.008244
404.005212	-3.698800	74.013249
403.316306	-0.727010	74.018254
402.928825	-9.021037	74.023258
402.012473	-7.190922	74.028263
401.299032	-3.944004	74.033268
401.120577	-1.632257	74.038273
399.718877	2.243117	74.043278
399.104584	-0.754363	74.048282
398.638684	8.891440	74.053287
398.052358	7.822736	74.058292
397.599701	6.021568	74.063297
396.859213	12.141112	74.068302
396.275889	4.076971	74.073306
395.388739	-5.047287	74.078311
394.413036	6.811663	74.083316
393.862860	2.676512	74.088321
393.413985	1.319418	74.093326
393.063326	-2.432809	74.098330
391.964868	-6.337099	74.103335
391.086068	-2.231247	74.108340
390.894574	-7.210401	74.113345
390.441631	-1.158755	74.118350
389.623258	-6.159440	74.123354
389.043343	-7.036785	74.128359
388.021603	3.285754	74.133364
387.176408	-4.113792	74.138369
386.371469	3.782104	74.143374
386.172112	-0.345871	74.148378
385.538770	-0.222857	74.153383
384.858062	6.465870	74.158388
384.372172	-2.738092	74.163393
383.201167	6.192214	74.168398
382.956525	0.559245	74.173402
382.596183	-2.011945	74.178407
381.545341	2.037752	74.183412
380.865348	-5.859597	74.188417
380.190683	4.013425	74.193422
379.000348	2.919555	74.198426
378.236150	4.522018	74.203431
377.891664	9.931951	74.208436
377.532125	-2.447443	74.213441
377.209088	11.065714	74.218446
376.847447	6.796450	74.223450
375.753016	-0.546033	74.228455
375.117477	2.983353	74.233460
374.593053	-0.681261	74.238465
373.244978	13.403645	74.243470
372.852622	5.250735	74.248474
372.343654	5.245130	74.253479
371.330206	10.580323	74.258484
371.049670	0.315526	74.263489
370.223267	10.126006	74.268494
369.865904	0.633499	74.273498
368.926765	-4.489851	74.278503
368.366550	4.286362	74.283508
368.100716	-4.870663	74.288513
366.984310	-3.409179	74.293518
365.985695	1.655583	74.298522
365.211166	1.804255	74.303527
364.941659	4.371773	74.308532
364.889563	3.514396	74.313537
364.273486	3.465939	74.318542
363.376838	-5.700942	74.323546
362.035672	-5.602314	74.328551
360.855593	11.226366	74.333556
360.602515	-2.474053	74.338561
360.036526	2.802452	74.343566
359.908306	-0.800723	74.348570
359.925337	-5.526115	74.353575
358.701660	-2.568439	74.358580
358.173905	-6.007026	74.363585
356.993700	3.683225	74.368590
356.023396	5.328001	74.373594
355.365398	-3.712915	74.378599
355.004814	1.576586	74.383604
354.582845	-3.446257	74.388609
353.696842	7.029696	74.393614
352.971149	-0.287962	74.398618
352.359543	-4.564690	74.403623
351.838625	1.355877	74.408628
351.567379	-3.240003	74.413633
350.409859	-4.462083	74.418638
349.983018	6.527290	74.423642
349.326693	-5.002175	74.428647
348.207936	5.181305	74.433652
347.480210	-1.469014	74.438657
346.686223	8.645368	74.443662
346.838955	0.024003	74.448666
346.176262	5.546143	74.453671
345.024374	8.161247	74.458676
344.817812	-0.943724	74.463681
344.185442	6.617195	74.468686
343.130724	-3.907394	74.473690
342.421570	-2.985435	74.478695
341.658110	5.197159	74.483700
341.562134	-1.725713	74.488705
340.503592	12.024497	74.493710
339.585828	-1.798635	74.498714
339.567837	-10.039571	74.503719
338.590242	10.225936	74.508724
337.986375	5.391344	74.513729
336.904289	8.123053	74.518734
336.574133	4.280840	74.523738
336.140973	-0.913671	74.528743
335.013508	0.494400	74.533748
334.792172	-12.028417	74.538753
333.793005	4.079191	74.543758
333.680811	-0.400117	74.548762
332.445089	2.729793	74.553767
331.392155	10.551695	74.558772
331.362225	-1.733567	74.563777
330.787837	9.079062	74.568782
330.241890	2.628422	74.573786
329.747574	-0.880139	74.578791
328.534017	5.615991	74.583796
328.183772	2.729405	74.588801
327.056372	5.372150	74.593806
326.581096	-2.371736	74.598810
326.335450	3.514426	74.603815
325.341582	4.309887	74.608820
324.744894	0.989520	74.613825
324.029804	8.595164	74.618830
323.551695	-2.218417	74.623834
322.959337	7.587885	74.628839
321.901938	9.992410	74.633844
321.557641	-1.878495	74.638849
320.920975	-1.168343	74.643854
319.833207	-3.142649	74.648858
318.969916	-5.824471	74.653863
318.271877	-1.871976	74.658868
318.073228	-10.604482	74.663873
317.730832	1.711761	74.668878
317.039097	-3.878325	74.673882
316.248389	0.314431	74.678887
315.658495	2.746945	74.683892
314.643681	3.430638	74.688897
313.911130	10.521858	74.693902
313.276395	5.903493	74.698906
313.363804	3.975271	74.703911
312.462167	7.813570	74.708916
311.645381	4.832618	74.713921
310.677103	7.601389	74.718926
310.118512	0.761710	74.723930
309.097836	9.161916	74.728935
308.393431	6.852141	74.733940
308.333665	5.354206	74.738945
307.776074	6.851226	74.743950
307.357290	-3.997034	74.748954
306.494061	-1.729101	74.753959
305.613469	-0.196370	74.758964
305.050506	-8.985921	74.763969
303.905772	-6.830808	74.768974
303.257800	6.221651	74.773978
302.773705	-4.013838	74.778983
302.328503	6.746666	74.783988
301.546952	-1.572837	74.788993
300.651310	1.911292	74.793998
300.482336	8.504285	74.799002
300.273453	-1.893332	74.804007
298.587210	6.855790	74.809012
298.199178	-6.279083	74.814017
297.503735	2.510807	74.819022
297.315150	-1.748176	74.824026
296.635302	-3.054246	74.829031
295.557860	5.448043	74.834036
295.201933	-5.908518	74.839041
293.929369	1.948397	74.844046
293.406933	-5.466283	74.849050
292.941917	3.397263	74.854055
292.537287	5.599993	74.859060
291.843007	4.067579	74.864065
290.705429	11.535578	74.869070
290.198614	3.831416	74.874074
290.144174	0.423056	74.879079
289.140360	0.720252	74.884084
288.603445	-8.087637	74.889089
287.637984	2.963931	74.894094
287.479115	2.877313	74.899098
286.459197	-3.130359	74.904103
285.625626	1.124427	74.909108
285.511517	-4.076771	74.914113
284.398453	0.753963	74.919118
283.816397	1.362386	74.924122
283.527356	-9.249515	74.929127
282.049807	3.252388	74.934132
281.488737	-7.022860	74.939137
280.785516	7.539579	74.944142
280.341466	1.913179	74.949146
280.202378	-9.690812	74.954151
278.965769	0.457860	74.959156
278.392113	-4.249070	74.964161
277.927172	-7.714993	74.969166
277.294324	-5.092710	74.974170
276.472195	-4.564286	74.979175
275.665306	6.070953	74.984180
275.470791	-13.741213	74.989185
274.749720	0.869793	74.994190
273.766662	3.085879	74.999194
273.312955	-2.624129	75.004199
272.433641	7.141191	75.009204
271.745204	3.062801	75.014209
270.606942	5.683649	75.019214
270.152498	3.565844	75.024218
269.937641	1.066096	75.029223
269.302283	0.172386	75.034228
269.046389	-4.067980	75.039233
268.010241	-4.935650	75.044238
267.129123	-2.217025	75.049242
266.834859	0.057997	75.054247
265.706372	-1.004676	75.059252
265.298174	-3.101467	75.064257
264.631385	-1.818831	75.069262
264.274861	-8.454172	75.074266
263.179797	-7.268841	75.079271
262.330783	4.628293	75.084276
262.239646	0.297014	75.089281
261.396595	10.543808	75.094286
260.553334	0.218931	75.099290
259.897785	9.092354	75.104295
259.290950	-1.757457	75.109300
259.080898	-10.281566	75.114305
257.735607	-3.556267	75.119310
257.387376	3.084218	75.124314
257.213362	-1.039895	75.129319
255.804707	11.996639	75.134324
255.382418	-4.349557	75.139329
254.629998	8.760558	75.144334
254.101294	-2.439152	75.149338
253.161490	-2.842808	75.154343
252.261330	1.838892	75.159348
252.213364	-5.208308	75.164353
251.608411	9.414161	75.169358
250.754282	-2.783864	75.174362
249.879941	-2.783240	75.179367
248.980458	-1.551812	75.184372
249.041486	3.243165	75.189377
248.129252	4.137601	75.194382
247.090593	-4.965591	75.199386
246.684803	-5.708241	75.204391
246.144088	0.111423	75.209396
245.905263	-2.884365	75.214401
244.948873	8.411763	75.219406
244.306025	-0.614184	75.224410
243.742853	-6.226313	75.229415
242.767447	0.722291	75.234420
242.237777	-2.794804	75.239425
241.727786	0.742980	75.244430
240.765067	0.782925	75.249434
239.929938	-3.226341	75.254439
239.260725	1.924722	75.259444
239.270803	-9.491741	75.264449
238.207247	2.029612	75.269454
237.121279	2.051360	75.274458
236.705609	1.576775	75.279463
236.096180	4.654201	75.284468
235.857160	4.440023	75.289473
234.837900	6.646125	75.294478
233.911077	-3.386313	75.299482
234.097073	0.075219	75.304487
232.850455	8.837875	75.309492
232.260851	-9.495283	75.314497
231.520390	4.125402	75.319502
231.052923	2.282478	75.324506
230.451947	4.879193	75.329511
229.502584	6.927508	75.334516
229.058967	-2.778279	75.339521
228.679358	-1.322229	75.344526
227.842057	-1.923554	75.349530
227.052962	-3.052927	75.354535
226.042559	3.040299	75.359540
225.662837	-2.692529	75.364545
224.797870	-5.583770	75.369550
224.049369	3.078982	75.374554
223.697537	-3.123464	75.379559
223.013228	-8.153338	75.384564
222.288498	-8.458811	75.389569
221.425867	-1.338956	75.394574
221.028246	-4.508111	75.399578
220.615180	-5.162869	75.404583
219.317316	4.025826	75.409588
219.303409	-6.685111	75.414593
218.938428	-1.546276	75.419598
217.719763	-1.744625	75.424602
216.968017	0.836706	75.429607
216.550835	1.522933	75.434612
215.563413	-0.049454	75.439617
214.596234	-4.020314	75.444622
213.906578	1.580263	75.449626
213.597503	-6.699409	75.454631
213.016377	-0.882759	75.459636
212.924303	-1.281200	75.464641
211.809955	0.279366	75.469646
211.206531	5.489329	75.474650
211.012365	-2.409718	75.479655
209.571343	3.892501	75.484660
209.329353	-5.263561	75.489665
208.372064	6.567273	75.494670
207.782406	4.458421	75.499674
207.156285	4.769552	75.504679
206.030819	15.878197	75.509684
205.879721	2.938947	75.514689
205.448751	8.596055	75.519694
204.794315	3.908329	75.524698
204.303048	11.240212	75.529703
203.444224	6.627645	75.534708
202.357926	1.441099	75.539713
201.219847	8.379385	75.544718
200.654053	9.477214	75.549722
200.894464	10.277794	75.554727
200.365785	20.258462	75.559732
199.321694	5.217702	75.564737
198.477072	9.851147	75.569742
197.707705	3.669538	75.574746
196.854244	6.967216	75.579751
195.912236	5.609934	75.584756
195.885218	0.027452	75.589761
195.183524	8.045700	75.594766
195.322744	2.439869	75.599770
194.603658	3.644134	75.604775
193.680696	6.623329	75.609780
192.832463	8.182478	75.614785
191.573871	11.106379	75.619790
191.143057	0.627475	75.624794
191.053800	4.583867	75.629799
189.892624	7.353474	75.634804
189.011456	1.112428	75.639809
188.538961	-0.253474	75.644814
188.104272	6.210001	75.649818
187.789923	1.100656	75.654823
186.617383	8.848640	75.659828
185.916383	3.603828	75.664833
185.343775	7.755543	75.669838
184.591247	13.030284	75.674842
184.070061	3.157110	75.679847
183.200583	2.603506	75.684852
183.110179	-0.294519	75.689857
182.220702	1.209710	75.694862
181.116672	8.415372	75.699866
180.881920	1.886780	75.704871
179.826323	9.430054	75.709876
179.260257	2.481225	75.714881
178.486144	3.661153	75.719886
177.743769	-2.702933	75.724890
177.645875	-0.388250	75.729895
176.785643	9.681540	75.734900
176.114838	7.901005	75.739905
175.325699	14.679600	75.744910
175.018789	11.858666	75.749914
174.454467	7.211772	75.754919
173.300010	4.937525	75.759924
173.125363	11.769528	75.764929
172.198294	8.918166	75.769934
171.191352	3.034627	75.774938
170.485738	2.450171	75.779943
170.167782	10.241675	75.784948
169.681441	5.391551	75.789953
168.815490	8.235517	75.794958
167.803719	3.568507	75.799962
167.489279	8.497454	75.804967
166.931499	8.728318	75.809972
166.476946	2.406649	75.814977
165.579880	5.753864	75.819982
164.996481	0.595961	75.824986
164.258174	6.607982	75.829991
163.224381	8.338643	75.834996
162.671099	5.465534	75.840001
162.297121	18.330842	75.845006
161.850618	5.979560	75.850010
160.949528	14.242485	75.855015
159.999540	6.943311	75.860020
159.981577	3.622178	75.865025
159.069469	4.035685	75.870030
158.081642	1.276013	75.875034
157.492189	0.428628	75.880039
156.902327	8.802769	75.885044
156.838790	-0.384891	75.890049
155.934746	0.123519	75.895054
155.162761	6.886766	75.900058
154.331703	-2.462354	75.905063
153.020864	4.038321	75.910068
152.821471	7.876664	75.915073
152.077058	8.506272	75.920078
151.887804	9.264972	75.925082
151.280869	10.385140	75.930087
150.178390	7.038238	75.935092
149.752937	3.383130	75.940097
149.234010	14.861836	75.945102
148.397553	14.979450	75.950106
147.647190	7.468692	75.955111
146.854548	16.129045	75.960116
146.594322	7.764324	75.965121
145.581544	3.654115	75.970126
144.760804	11.923155	75.975130
144.324149	12.987791	75.980135
143.964070	15.924564	75.985140
143.003080	4.606165	75.990145
142.039467	12.008638	75.995150
141.818646	13.953440	76.000154
141.384896	8.174051	76.005159
140.475767	14.093477	76.010164
139.814831	5.012105	76.015169
139.043846	12.858500	76.020174
138.571047	6.085611	76.025178
137.619750	9.613360	76.030183
136.840356	13.028551	76.035188
136.694347	4.785963	76.040193
136.147954	5.153781	76.045198
135.100848	7.742809	76.050202
134.293039	8.798821	76.055207
133.792274	0.218586	76.060212
133.397082	13.421566	76.065217
132.476466	11.042248	76.070222
131.682708	19.075195	76.075226
131.339638	8.572851	76.080231
130.385173	15.751534	76.085236
129.540916	9.451012	76.090241
128.897367	13.402752	76.095246
128.654288	7.354858	76.100250
128.376574	2.212875	76.105255
127.175682	2.147347	76.110260
126.643935	2.487603	76.115265
125.911520	9.722336	76.120270
125.369621	3.348377	76.125274
124.659540	4.995899	76.130279
123.571915	11.407386	76.135284
123.410911	9.946100	76.140289
122.785118	12.825901	76.145294
121.985004	12.158762	76.150298
121.337225	7.842138	76.155303
120.860700	22.775293	76.160308
120.106479	10.301209	76.165313
119.161370	14.479221	76.170318
118.570833	13.083271	76.175322
118.353421	14.833577	76.180327
117.180732	22.516968	76.185332
116.627960	10.572125	76.190337
115.870533	6.676663	76.195342
115.042270	14.346128	76.200346
114.527285	1.641531	76.205351
113.638717	7.384229	76.210356
113.481460	5.174916	76.215361
112.981341	20.293170	76.220366
112.100258	13.482892	76.225370
111.253005	3.306942	76.230375
110.611333	7.006088	76.235380
110.431358	10.986408	76.240385
109.231174	16.236361	76.245390
108.374647	18.911700	76.250394
108.315458	11.768530	76.255399
107.690046	15.408319	76.260404
106.655764	2.595729	76.265409
105.915541	13.234570	76.270414
105.362461	14.108056	76.275418
105.311392	6.939940	76.280423
104.070462	11.385888	76.285428
103.572384	3.822304	76.290433
103.005179	16.291095	76.295438
101.969948	4.971941	76.300442
101.293276	10.209376	76.305447
100.762005	8.759829	76.310452
100.443296	9.349953	76.315457
99.336004	2.895859	76.320462
98.288612	3.909667	76.325466
98.115803	6.878078	76.330471
97.496993	7.952847	76.335476
97.268176	11.076838	76.340481
96.395044	9.568271	76.345486
95.601887	12.110513	76.350490
95.189286	10.121680	76.355495
93.973082	10.394481	76.360500
93.278449	10.990939	76.365505
92.633566	4.956666	76.370510
92.124771	2.650459	76.375514
91.444284	2.695915	76.380519
90.456034	14.856556	76.385524
90.239964	12.188296	76.390529
89.878102	7.002970	76.395534
89.294851	9.500702	76.400538
88.387777	5.487196	76.405543
87.549838	13.350588	76.410548
87.148825	2.436479	76.415553
85.990849	11.571391	76.420558
85.441946	3.788851	76.425562
85.109637	6.628165	76.430567
84.305935	6.838344	76.435572
83.544380	2.117280	76.440577
83.025846	4.800222	76.445582
82.349791	10.477506	76.450586
82.129752	8.934179	76.455591
81.094353	17.762562	76.460596
80.810156	0.503478	76.465601
79.661935	10.899898	76.470606
78.617543	16.199133	76.475610
78.280251	4.522703	76.480615
77.698357	7.496431	76.485620
77.192308	13.392595	76.490625
76.049473	0.947398	76.495630
75.210494	6.822540	76.500634
75.344449	-0.813440	76.505639
74.500169	5.735864	76.510644
73.998089	-0.499357	76.515649
73.343262	14.815440	76.520654
72.418608	2.013771	76.525658
71.566202	2.491902	76.530663
70.249672	5.368333	76.535668
69.920846	-1.919472	76.540673
69.508487	3.212742	76.545678
68.929937	-1.274165	76.550682
68.884195	9.285465	76.555687
67.396553	12.491944	76.560692
67.127355	-0.444209	76.565697
66.312223	2.524141	76.570702
66.176584	-0.442351	76.575706
66.000853	7.017411	76.580711
64.779755	16.343739	76.585716
64.251573	1.848377	76.590721
62.933539	4.658824	76.595726
62.426776	3.131266	76.600730
62.212376	1.686385	76.605735
60.796937	14.656282	76.610740
60.297779	15.119080	76.615745
59.717760	9.236889	76.620750
59.047584	11.097248	76.625754
58.716754	8.116155	76.630759
58.008742	8.404116	76.635764
57.247398	4.823094	76.640769
56.936495	13.382986	76.645774
55.563720	12.113380	76.650778
55.488238	5.151001	76.655783
54.528264	14.148700	76.660788
53.914997	-2.679446	76.665793
53.021550	0.033332	76.670798
52.298445	2.373613	76.675802
52.168990	-3.802763	76.680807
51.591245	13.923368	76.685812
50.729717	7.567290	76.690817
49.864090	9.884573	76.695822
49.068879	7.376487	76.700826
48.960389	2.571782	76.705831
47.369368	16.725524	76.710836
47.052234	7.764386	76.715841
46.119378	13.810620	76.720846
45.991858	9.619192	76.725850
45.875558	8.062479	76.730855
44.932002	9.471309	76.735860
44.349942	1.878562	76.740865
43.399212	0.675688	76.745870
42.279304	6.709176	76.750874
41.868715	-2.978171	76.755879
41.035124	3.654587	76.760884
40.748043	-4.188614	76.765889
40.439623	6.802387	76.770894
39.674015	-2.432549	76.775898
39.515553	4.682280	76.780903
37.911793	12.543250	76.785908
37.102997	0.052687	76.790913
36.759738	3.716870	76.795918
36.419422	6.606349	76.800922
35.575234	-1.329339	76.805927
34.492434	14.842146	76.810932
33.918775	10.543688	76.815937
33.581882	-2.786909	76.820942
32.422619	-0.801235	76.825946
31.631119	-0.181427	76.830951
31.187477	2.224669	76.835956
31.215832	1.147903	76.840961
30.396143	1.543564	76.845966
29.432916	2.252259	76.850970
29.043707	-1.731857	76.855975
28.124139	10.141893	76.860980
27.199735	6.039719	76.865985
26.506626	7.318731	76.870990
25.865367	4.885440	76.875994
25.905573	1.802602	76.880999
24.972754	6.792341	76.886004
24.113783	0.511558	76.891009
23.439160	5.706106	76.896014
23.360080	7.905834	76.901018
22.469679	2.639252	76.906023
21.482028	3.635680	76.911028
21.042499	1.089797	76.916033
19.752894	1.975123	76.921038
19.184381	4.699162	76.926042
18.652948	12.590951	76.931047
18.364135	11.127981	76.936052
18.158401	-3.336790	76.941057
16.874917	-0.640634	76.946062
15.819147	4.255184	76.951066
15.642893	-3.342355	76.956071
15.063659	15.653385	76.961076
14.204307	-2.220372	76.966081
13.459813	-0.270882	76.971086
13.089626	8.710022	76.976090
12.646346	9.436714	76.981095
11.380101	11.858906	76.986100
10.722005	4.379215	76.991105
10.181717	6.110067	76.996110
10.086590	3.192307	77.001114
9.380880	4.072812	77.006119
8.223045	10.355201	77.011124
7.956124	-3.385493	77.016129
6.643507	6.800642	77.021134
5.879894	-1.474294	77.026139
5.745635	-3.980559	77.031143
4.933813	9.273103	77.036148
4.923731	0.181008	77.041153
4.048193	9.389165	77.046158