Tue Jun 21 12:24:19 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.655721	90.144538	0.000000
0.403979	82.076501	0.005005
0.725058	86.158186	0.010010
0.469578	87.266012	0.015014
0.774950	80.659530	0.020019
0.640677	82.051771	0.025024
0.593766	64.756234	0.030029
0.587667	59.389485	0.035034
-0.378043	54.412524	0.040038
-0.567601	44.093881	0.045043
-0.794846	27.330462	0.050048
-1.406820	20.308777	0.055053
-1.514345	23.006086	0.060058
-1.674656	12.761752	0.065062
-1.931964	6.106399	0.070067
-2.435173	0.979460	0.075072
-2.669572	-0.469107	0.080077
-2.520414	-6.693892	0.085082
-3.595072	-2.078397	0.090086
-3.779493	0.900607	0.095091
-3.876706	-0.528448	0.100096
-4.325030	8.586519	0.105101
-4.108274	-2.349934	0.110106
-4.487141	7.859384	0.115110
-5.423730	-3.196880	0.120115
-5.531833	-3.451382	0.125120
-6.106688	2.921480	0.130125
-5.715908	-8.257302	0.135130
-5.799055	5.406098	0.140134
-5.873853	-1.562844	0.145139
-5.818613	-0.879240	0.150144
-6.214176	-4.004101	0.155149
-6.883567	-8.937757	0.160154
-7.256207	1.105161	0.165158
-7.741073	-7.522537	0.170163
-7.347576	-2.706359	0.175168
-7.510599	-1.489726	0.180173
-7.872741	1.910019	0.185178
-8.609818	6.942228	0.190182
-8.592750	1.278427	0.195187
-8.889680	0.710256	0.200192
-9.185872	-0.655854	0.205197
-8.947842	-9.668277	0.210202
-10.145860	0.872242	0.215206
-10.392852	-6.067000	0.220211
-10.581990	-5.508885	0.225216
-10.783835	-4.537621	0.230221
-10.604617	-9.699417	0.235226
-10.557718	-2.446800	0.240230
-10.641833	-3.598205	0.245235
-10.856398	-13.369212	0.250240
-11.717606	-2.880720	0.255245
-11.921981	-16.594150	0.260250
-12.526203	1.739574	0.265254
-12.265579	-7.349210	0.270259
-12.067901	-6.318010	0.275264
-12.364842	-9.733691	0.280269
-13.263949	-4.712936	0.285274
-13.623233	-0.196563	0.290278
-13.398622	-2.297351	0.295283
-13.622598	-11.213336	0.300288
-14.531635	2.156837	0.305293
-14.621473	3.612950	0.310298
-15.349949	-4.343534	0.315302
-15.333522	-4.565377	0.320307
-15.374436	-4.117055	0.325312
-15.447493	-2.542559	0.330317
-15.271820	-13.834109	0.335322
-15.521796	1.320727	0.340326
-15.307421	-0.600965	0.345331
-16.584665	-6.609275	0.350336
-16.810665	3.511777	0.355341
-16.792546	-6.936926	0.360346
-16.798147	-0.923350	0.365350
-17.146936	-1.441098	0.370355
-17.950231	-5.215348	0.375360
-18.416982	3.138792	0.380365
-18.414161	-6.802009	0.385370
-18.662401	-0.974396	0.390374
-18.451566	0.865269	0.395379
-18.275990	-5.815389	0.400384
-18.785946	1.910296	0.405389
-19.103316	-4.060423	0.410394
-19.834152	-2.344046	0.415398
-19.755274	-1.084394	0.420403
-19.846364	-6.028171	0.425408
-20.557519	8.657219	0.430413
-20.945523	8.500178	0.435418
-21.341514	6.717844	0.440422
-21.420432	6.001683	0.445427
-21.385310	4.591759	0.450432
-21.537983	5.153309	0.455437
-21.231773	-0.547519	0.460442
-22.094940	3.409979	0.465446
-22.333612	-1.739252	0.470451
-22.639919	1.081547	0.475456
-22.990768	-1.404847	0.480461
-22.945403	-2.371481	0.485466
-23.199879	-2.411119	0.490470
-23.941614	-5.545943	0.495475
-24.168090	-1.074651	0.500480
-24.270530	10.864100	0.505485
-24.289560	-4.282674	0.510490
-24.236953	2.296094	0.515494
-24.734574	-1.297303	0.520499
-25.316203	0.752329	0.525504
-26.102544	9.342324	0.530509
-25.913039	0.383910	0.535514
-25.907958	3.622007	0.540518
-26.024862	3.952082	0.545523
-26.220028	2.175564	0.550528
-26.466996	0.984429	0.555533
-27.135071	2.160971	0.560538
-27.559556	8.134792	0.565542
-27.938554	1.380603	0.570547
-27.697261	-0.483386	0.575552
-27.806478	2.249127	0.580557
-27.683247	-6.228655	0.585562
-27.923854	5.932870	0.590566
-28.592968	1.029757	0.595571
-29.077133	2.609581	0.600576
-29.163812	3.761870	0.605581
-29.168409	0.271531	0.610586
-29.381364	3.104894	0.615590
-30.098967	0.164394	0.620595
-30.506763	3.209792	0.625600
-31.331144	-1.402984	0.630605
-30.828972	-0.739718	0.635610
-31.340205	2.591577	0.640614
-30.851922	-0.604859	0.645619
-30.901608	-1.227193	0.650624
-31.099304	2.434414	0.655629
-31.410869	-3.673820	0.660634
-32.198792	-3.498826	0.665638
-32.323438	-1.967093	0.670643
-32.285184	-9.401710	0.675648
-32.980278	2.417717	0.680653
-33.360547	-5.903278	0.685658
-33.887053	-0.171071	0.690662
-33.782595	2.867247	0.695667
-33.814633	-8.209743	0.700672
-34.041625	2.809927	0.705677
-33.888221	-11.803586	0.710682
-35.067188	-1.445397	0.715686
-35.456062	-7.257062	0.720691
-35.545627	-11.304803	0.725696
-35.531238	-3.015544	0.730701
-35.571886	-9.028138	0.735706
-35.791255	-1.892452	0.740710
-35.556169	-0.753587	0.745715
-36.231381	-2.436596	0.750720
-36.963745	-4.995376	0.755725
-37.045537	3.762496	0.760730
-37.341480	-0.460244	0.765734
-37.245412	1.239968	0.770739
-37.261992	-7.717859	0.775744
-38.369066	-4.731299	0.780749
-38.508488	-7.621518	0.785754
-38.791025	-10.122971	0.790758
-39.207042	-3.847453	0.795763
-39.063072	-3.216037	0.800768
-39.271566	-5.207609	0.805773
-39.036263	-6.640421	0.810778
-39.119904	0.770367	0.815782
-39.600035	-5.950097	0.820787
-39.926938	-2.523430	0.825792
-40.424993	5.465897	0.830797
-40.538567	3.000397	0.835802
-41.385128	1.420356	0.840806
-41.815138	-4.612219	0.845811
-41.651843	3.128860	0.850816
-42.176383	-3.336006	0.855821
-41.974574	-2.232478	0.860826
-42.403909	-0.666864	0.865830
-42.377073	-4.851295	0.870835
-42.334004	-3.304713	0.875840
-42.561453	-1.471796	0.880845
-43.098335	-5.194454	0.885850
-43.689418	0.101292	0.890854
-44.126927	-0.944821	0.895859
-43.974640	6.870701	0.900864
-44.024038	8.372016	0.905869
-43.824397	1.265473	0.910874
-44.733249	4.067066	0.915878
-45.079890	5.171041	0.920883
-45.061709	6.756476	0.925888
-45.249616	16.042823	0.930893
-45.415799	0.714204	0.935898
-46.079797	7.320083	0.940902
-46.595221	-2.082212	0.945907
-46.475233	4.548543	0.950912
-46.695445	2.768873	0.955917
-46.700464	-6.784248	0.960922
-46.639162	-2.856708	0.965926
-47.625714	3.409104	0.970931
-48.211782	3.365378	0.975936
-48.014462	5.514132	0.980941
-48.023759	-3.302428	0.985946
-48.294557	-2.178650	0.990950
-48.473691	-0.752347	0.995955
-48.780490	1.290452	1.000960
-49.650540	12.059450	1.005965
-49.464774	1.384464	1.010970
-49.743023	-0.882478	1.015974
-49.858987	-10.888849	1.020979
-49.874287	-3.587258	1.025984
-50.777850	-4.280712	1.030989
-51.038972	-4.722399	1.035994
-51.391414	0.083711	1.040998
-51.429435	-5.433224	1.046003
-51.420616	-7.540901	1.051008
-51.432265	-3.854853	1.056013
-51.332250	-4.956435	1.061018
-52.010274	-1.961794	1.066022
-52.548542	1.250054	1.071027
-52.712975	-4.269626	1.076032
-52.919383	0.819942	1.081037
-53.062564	-3.379155	1.086042
-53.966809	-0.461109	1.091046
-54.307978	-0.594527	1.096051
-54.258538	0.552783	1.101056
-53.998083	-0.713700	1.106061
-54.449466	-0.491032	1.111066
-54.899574	-5.071064	1.116070
-54.791654	5.150778	1.121075
-54.666701	1.058432	1.126080
-55.631555	-7.285724	1.131085
-55.807889	-8.813364	1.136090
-56.181352	0.405233	1.141094
-56.212456	0.049970	1.146099
-56.078965	1.534613	1.151104
-56.739666	-4.451862	1.156109
-57.316828	-3.896775	1.161114
-57.712739	-4.393297	1.166118
-57.695712	-0.422510	1.171123
-57.686455	-4.791496	1.176128
-57.771142	1.665164	1.181133
-57.881884	-6.988962	1.186138
-58.104821	-5.575138	1.191142
-58.993796	-3.406326	1.196147
-58.998038	-3.920352	1.201152
-59.227181	1.470954	1.206157
-59.445492	-8.271604	1.211162
-59.485942	0.108827	1.216166
-60.142435	-2.976170	1.221171
-60.641648	-0.483160	1.226176
-61.085437	6.136966	1.231181
-61.119657	-8.009962	1.236186
-60.894518	-1.429382	1.241190
-60.998312	-3.049942	1.246195
-60.890051	-6.119706	1.251200
-61.405127	-1.933519	1.256205
-62.182901	-3.195993	1.261210
-62.663273	2.041362	1.266214
-62.864504	0.899881	1.271219
-62.891164	-5.228101	1.276224
-62.881454	-4.536958	1.281229
-62.696361	3.023106	1.286234
-63.324221	-2.567431	1.291238
-63.830862	0.659703	1.296243
-64.187088	-1.847305	1.301248
-64.380376	13.708997	1.306253
-64.464331	5.014712	1.311258
-64.455175	-7.819242	1.316262
-65.313157	5.217080	1.321267
-65.376213	-5.456159	1.326272
-66.021979	2.054431	1.331277
-65.821848	-8.386521	1.336282
-65.841928	3.285994	1.341286
-66.055152	-1.063710	1.346291
-65.973222	-1.588652	1.351296
-66.829392	10.629233	1.356301
-67.142540	-1.917706	1.361306
-67.447885	6.272757	1.366310
-67.678511	4.991697	1.371315
-67.604749	-0.076862	1.376320
-67.724794	0.268732	1.381325
-68.100201	-9.550815	1.386330
-68.837377	-0.459056	1.391334
-69.147180	-0.831112	1.396339
-69.234355	-6.557760	1.401344
-69.520611	4.953808	1.406349
-69.031570	-3.389590	1.411354
-69.363691	7.072070	1.416358
-69.736732	-0.262270	1.421363
-70.191636	-3.577588	1.426368
-70.689713	0.110676	1.431373
-70.376208	1.098025	1.436378
-70.900316	-6.203992	1.441382
-71.519878	-1.977807	1.446387
-71.685837	1.548501	1.451392
-72.174978	5.110968	1.456397
-72.007914	1.030592	1.461402
-72.291051	3.674496	1.466406
-72.415510	-5.246914	1.471411
-72.128235	0.686188	1.476416
-73.000921	4.459778	1.481421
-73.378084	8.489534	1.486426
-73.351966	-0.359530	1.491430
-73.964978	5.127910	1.496435
-73.807825	-1.173384	1.501440
-74.814153	-1.408972	1.506445
-75.102683	3.987236	1.511450
-74.757401	0.541765	1.516454
-75.027621	0.217420	1.521459
-75.096755	-1.558062	1.526464
-75.532373	5.186806	1.531469
-75.267844	-3.579393	1.536474
-76.058835	3.792055	1.541478
-76.440609	10.350014	1.546483
-76.590982	6.545786	1.551488
-77.167671	-0.212949	1.556493
-76.876865	1.633991	1.561498
-77.014138	9.899431	1.566502
-77.212119	0.988419	1.571507
-77.909528	4.785473	1.576512
-78.359320	-0.814819	1.581517
-78.535988	-3.394976	1.586522
-78.461092	-3.485410	1.591526
-78.633496	2.794167	1.596531
-78.634171	-2.485247	1.601536
-79.361053	0.972934	1.606541
-79.734461	-8.324800	1.611546
-80.109176	-0.321960	1.616550
-80.624649	5.513208	1.621555
-80.403481	1.152342	1.626560
-80.238324	5.057552	1.631565
-80.403533	0.756136	1.636570
-80.930351	10.694748	1.641574
-81.770646	2.485069	1.646579
-81.609829	-2.995728	1.651584
-81.967324	9.244156	1.656589
-81.670856	-4.521827	1.661594
-81.973148	4.508570	1.666598
-82.248587	7.322288	1.671603
-82.890635	3.871611	1.676608
-83.239277	6.850188	1.681613
-83.429655	0.794311	1.686618
-83.659574	4.857302	1.691622
-83.363552	6.444477	1.696627
-83.942750	-4.776127	1.701632
-84.691279	4.707052	1.706637
-84.351102	-3.480270	1.711642
-84.719506	9.339014	1.716646
-85.054793	0.068115	1.721651
-85.248139	-1.168995	1.726656
-85.949339	-0.193566	1.731661
-86.267439	3.754776	1.736666
-86.583729	8.791504	1.741670
-86.718868	7.133512	1.746675
-86.550910	-4.385273	1.751680
-87.193702	-4.130902	1.756685
-87.059376	0.836524	1.761690
-87.078237	6.196557	1.766694
-86.918042	-1.221354	1.771699
-87.603089	3.057513	1.776704
-87.981633	12.420814	1.781709
-87.921286	-2.972738	1.786714
-88.213112	4.258027	1.791718
-89.108518	1.093215	1.796723
-89.183730	-3.592313	1.801728
-89.725804	3.332196	1.806733
-89.686253	3.169077	1.811738
-89.987172	6.630517	1.816742
-90.291598	-1.510631	1.821747
-89.871947	2.956663	1.826752
-90.458864	8.572194	1.831757
-90.590172	5.583149	1.836762
-91.547157	6.376179	1.841766
-91.807070	5.478258	1.846771
-91.595338	0.072894	1.851776
-91.669324	2.467067	1.856781
-91.951079	10.726639	1.861786
-91.531999	8.074851	1.866790
-92.406592	-2.342821	1.871795
-92.695892	0.115427	1.876800
-93.055528	2.230915	1.881805
-93.077471	3.005839	1.886810
-93.706569	-1.811338	1.891814
-94.483309	-2.497765	1.896819
-94.385395	-3.644782	1.901824
-94.690764	3.061150	1.906829
-94.893878	5.150518	1.911834
-94.595272	3.112261	1.916838
-94.861548	4.200562	1.921843
-94.700801	-2.787254	1.926848
-95.502534	4.403245	1.931853
-95.902500	2.527647	1.936858
-96.363560	2.265892	1.941862
-96.558380	0.089525	1.946867
-96.405884	-7.803863	1.951872
-96.388282	-3.753452	1.956877
-97.010477	-4.330301	1.961882
-97.508870	1.872037	1.966886
-97.770282	9.960704	1.971891
-97.600103	-7.175130	1.976896
-97.913366	3.840473	1.981901
-97.931987	-5.522530	1.986906
-98.613458	3.297950	1.991910
-99.419246	6.768019	1.996915
-99.383021	4.016722	2.006912
-98.633144	6.855353	2.016909
-98.239860	3.565455	2.026906
-98.062401	1.667924	2.036902
-97.550683	-4.034346	2.046899
-97.027285	-0.590940	2.056896
-96.348569	-0.480638	2.066893
-95.722828	-3.824247	2.076890
-95.623184	-4.133344	2.086886
-94.488228	-4.415332	2.096883
-94.325608	-4.275473	2.106880
-93.852139	2.615177	2.116877
-93.300314	3.269305	2.126874
-92.469503	-2.715801	2.136870
-92.195001	-8.798059	2.146867
-92.216443	-2.354184	2.156864
-91.394255	-5.813510	2.166861
-91.168052	-3.581478	2.176858
-89.974120	-1.781791	2.186854
-89.588017	-1.828714	2.196851
-89.087325	-1.013581	2.206848
-89.216760	-0.953191	2.216845
-88.193329	-4.117656	2.226842
-87.707500	-1.868555	2.236838
-87.617440	-2.347965	2.246835
-86.875519	-0.158663	2.256832
-86.522157	-3.956262	2.266829
-85.708892	-1.522904	2.276826
-85.241701	-7.452529	2.286822
-84.864933	2.506041	2.296819
-83.892334	-0.618787	2.306816
-83.454376	-1.238008	2.316813
-83.404191	1.497579	2.326810
-83.077314	-2.744745	2.336806
-82.253911	0.012951	2.346803
-81.834416	-0.108260	2.356800
-81.431543	-6.681834	2.366797
-80.341970	-0.694624	2.376794
-80.170831	-3.534578	2.386790
-80.125733	-9.069468	2.396787
-79.162781	-9.680003	2.406784
-78.495002	4.233651	2.416781
-78.578437	2.655947	2.426778
-77.840230	5.419259	2.436774
-77.465840	-0.807777	2.446771
-76.723573	-2.270305	2.456768
-75.940901	-4.865564	2.466765
-75.665756	-4.531145	2.476762
-75.505514	-6.192870	2.486758
-74.521222	-1.065304	2.496755
-73.807508	0.804433	2.506752
-73.873496	-3.562312	2.516749
-73.713307	2.846942	2.526746
-73.002390	-1.266931	2.536742
-72.235894	-0.419745	2.546739
-71.388640	2.394268	2.556736
-70.809289	0.126689	2.566733
-70.903346	2.171893	2.576730
-70.883833	2.487000	2.586726
-69.886426	0.889354	2.596723
-69.423700	3.387290	2.606720
-68.427591	-1.346020	2.616717
-68.021439	0.584336	2.626714
-67.926172	1.499018	2.636710
-67.262210	4.324617	2.646707
-66.643431	2.743836	2.656704
-66.170425	2.144695	2.666701
-65.887809	2.369996	2.676698
-65.207959	0.631702	2.686694
-64.991014	2.880485	2.696691
-64.191023	-0.623570	2.706688
-63.355165	-2.854792	2.716685
-63.327145	3.111038	2.726682
-62.899664	-0.409570	2.736678
-62.089828	4.196222	2.746675
-61.734888	4.797208	2.756672
-61.344040	0.534806	2.766669
-60.350126	1.438185	2.776666
-60.066509	-3.354363	2.786662
-59.838678	-2.248440	2.796659
-59.713635	-6.809434	2.806656
-58.511645	-2.177105	2.816653
-58.376025	-0.708950	2.826650
-57.486711	-1.426627	2.836646
-56.912932	0.024684	2.846643
-56.930573	-0.256098	2.856640
-56.491468	3.565821	2.866637
-55.177783	-3.745222	2.876634
-55.098590	-6.271989	2.886630
-55.121951	2.752476	2.896627
-54.030148	-4.289066	2.906624
-53.501561	-5.305818	2.916621
-53.502222	-1.589492	2.926618
-52.421705	-0.463944	2.936614
-52.116294	-4.696586	2.946611
-52.076574	-0.793116	2.956608
-51.034863	-6.702296	2.966605
-50.678199	-2.923433	2.976602
-50.512254	-0.726665	2.986598
-49.566279	-2.846504	2.996595
-48.989466	0.761544	3.006592
-49.065114	-2.728497	3.016589
-48.018698	-5.830568	3.026586
-47.606318	-3.033447	3.036582
-47.624858	0.282569	3.046579
-46.389989	-5.454493	3.056576
-46.030831	-4.160679	3.066573
-46.121112	-2.744226	3.076570
-44.769687	-7.979753	3.086566
-44.530177	-2.800563	3.096563
-44.448128	-1.657654	3.106560
-43.943112	-3.673841	3.116557
-43.036998	1.274036	3.126554
-42.927881	1.043196	3.136550
-41.640109	-4.245809	3.146547
-41.421460	-5.810905	3.156544
-41.060359	-2.011040	3.166541
-41.190289	-6.372138	3.176538
-40.071138	-8.363967	3.186534
-39.666937	-1.775801	3.196531
-39.360733	-2.699413	3.206528
-38.354420	-5.682613	3.216525
-38.093155	-1.487048	3.226522
-38.111036	-10.997600	3.236518
-37.111975	-2.981202	3.246515
-36.354646	-1.424148	3.256512
-36.206014	-9.095487	3.266509
-35.666443	-6.530449	3.276506
-35.091880	2.476800	3.286502
-34.766207	3.713724	3.296499
-33.976687	-4.168075	3.306496
-33.079722	-3.495815	3.316493
-33.229663	1.993470	3.326490
-33.159647	2.197273	3.336486
-32.456537	2.498167	3.346483
-31.830609	6.900679	3.356480
-30.425428	3.184377	3.366477
-30.681930	-2.176291	3.376474
-30.378272	1.100793	3.386470
-30.000075	0.770859	3.396467
-28.928910	-2.886374	3.406464
-28.308698	-7.385131	3.416461
-28.303151	-1.885833	3.426458
-27.678992	-4.049587	3.436454
-27.177441	3.094867	3.446451
-26.868117	-5.718456	3.456448
-25.747049	1.357786	3.466445
-25.511699	1.051903	3.476442
-25.442766	0.343831	3.486438
-24.320469	-0.502323	3.496435
-23.701497	-0.539790	3.506432
-23.376654	1.988099	3.516429
-23.540808	-4.565472	3.526426
-23.349911	-0.173313	3.536422
-22.401576	-2.121835	3.546419
-21.429323	-5.775529	3.556416
-20.791198	-3.487029	3.566413
-20.683935	-3.125595	3.576410
-20.107008	-6.892836	3.586406
-19.476981	-5.753732	3.596403
-19.432072	1.807177	3.606400
-18.556995	-3.562658	3.616397
-17.858186	-3.687043	3.626394
-17.486148	-5.513457	3.636390
-17.358304	-5.319823	3.646387
-16.670122	0.113657	3.656384
-15.957033	-4.371435	3.666381
-15.631463	-2.922287	3.676378
-14.673655	-3.492438	3.686374
-14.543664	-0.476255	3.696371
-14.520749	-4.666265	3.706368
-13.514158	-9.764856	3.716365
-12.960570	-4.030691	3.726362
-12.953770	-2.666471	3.736358
-12.059842	-7.455955	3.746355
-11.202254	-4.173189	3.756352
-10.857360	-6.093110	3.766349
-10.757793	-13.243589	3.776346
-10.416475	-12.301089	3.786342
-9.153249	-9.437791	3.796339
-9.065584	-9.424024	3.806336
-8.914592	-6.887895	3.816333
-7.928042	-10.986149	3.826330
-7.622709	-8.584251	3.836326
-7.218818	-5.244928	3.846323
-5.812213	-14.645594	3.856320
-5.712503	-12.737001	3.866317
-5.899995	-13.372972	3.876314
-5.847026	-8.425876	3.886310
-4.868256	-4.864822	3.896307
-3.911277	-3.447914	3.906304
-3.410635	-1.852497	3.916301
-3.585362	4.065703	3.926298
-3.037741	11.856941	3.936294
-2.693529	22.506554	3.946291
-2.134386	44.178686	3.956288
-1.451885	58.315026	3.966285
-0.956495	78.111011	3.976282
-0.704257	94.154410	3.986278
-0.318543	113.550312	3.996275
0.000000	128.206070	4.001280
0.420693	134.949694	4.006285
0.480168	142.950170	4.011290
0.884118	161.333809	4.016294
0.829455	167.599482	4.021299
1.203518	175.385671	4.026304
1.120506	178.302331	4.031309
1.226302	170.404346	4.036314
1.089313	172.718008	4.041318
1.083865	170.197475	4.046323
1.370285	167.079823	4.051328
1.196595	174.228155	4.056333
1.761624	163.781320	4.061338
0.768447	168.482630	4.066342
1.044886	173.141239	4.071347
1.503794	167.013487	4.076352
1.117393	175.529253	4.081357
1.125889	170.719888	4.086362
1.042207	174.971237	4.091366
1.200673	164.548312	4.096371
1.063919	172.892692	4.101376
0.896168	192.755936	4.106381
1.663880	184.640392	4.111386
1.794189	196.124369	4.116390
1.225883	194.134333	4.121395
1.787569	190.030396	4.126400
1.680909	192.373967	4.131405
1.539177	174.730912	4.136410
1.473168	175.834206	4.141414
1.395581	178.194865	4.146419
1.487010	167.797247	4.151424
1.158806	182.336505	4.156429
1.731623	173.181315	4.161434
1.512891	172.894809	4.166438
1.361107	175.591581	4.171443
1.416127	177.249276	4.176448
1.399469	182.771220	4.181453
1.259777	186.307626	4.186458
1.420375	199.157478	4.191462
1.434248	201.530029	4.196467
1.728073	198.369901	4.201472
1.800257	203.719273	4.206477
1.682648	198.063492	4.211482
1.785637	205.277714	4.216486
1.716592	194.376214	4.221491
2.167168	200.555868	4.226496
1.515945	198.700529	4.231501
1.950235	187.085790	4.236506
1.843836	186.797456	4.241510
1.593373	178.705871	4.246515
1.665345	179.586811	4.251520
1.375416	185.627810	4.256525
1.990838	196.542656	4.261530
1.995441	197.951771	4.266534
1.875954	188.436425	4.271539
1.678780	182.628064	4.276544
1.759588	196.625607	4.281549
1.793422	185.358582	4.286554
1.695234	192.748390	4.291558
2.086428	199.488246	4.296563
1.929408	192.873431	4.301568
1.625883	195.885022	4.306573
1.779200	198.052538	4.311578
2.024215	207.537465	4.316582
2.152381	196.083130	4.321587
1.770352	192.223477	4.326592
1.780537	198.907037	4.331597
2.162045	202.121718	4.336602
2.015604	204.704931	4.341606
1.814159	198.980547	4.346611
1.724568	197.814640	4.351616
1.758725	205.537941	4.356621
1.688969	201.461208	4.361626
1.775665	203.024860	4.366630
1.819010	209.600910	4.371635
1.866086	206.690027	4.376640
1.913929	202.298606	4.381645
1.924007	204.672774	4.386650
1.810842	215.595406	4.391654
1.933595	211.704256	4.396659
2.119341	208.485457	4.401664
1.858146	216.653132	4.406669
2.133938	213.673984	4.411674
2.370589	231.042885	4.416678
2.678407	217.859921	4.421683
2.244370	214.563387	4.426688
1.794634	203.761230	4.431693
2.042682	199.388754	4.436698
1.853197	204.923143	4.441702
2.109129	220.857960	4.446707
2.232105	228.443821	4.451712
2.559459	233.240243	4.456717
2.478404	234.468184	4.461722
2.014258	227.935392	4.466726
2.212338	228.063139	4.471731
2.594650	233.253617	4.476736
2.281551	235.761029	4.481741
2.419643	220.443168	4.486746
2.363092	225.418996	4.491750
1.998697	209.529200	4.496755
2.461222	219.319111	4.501760
2.482959	235.641812	4.506765
2.645498	226.713977	4.511770
2.239459	217.079512	4.516774
2.368214	224.212910	4.521779
2.761017	217.659776	4.526784
2.731822	222.380062	4.531789
2.160606	207.231372	4.536794
2.097149	212.770549	4.541798
2.018091	234.603567	4.546803
2.596797	243.034344	4.551808
2.370669	239.262923	4.556813
2.407324	239.050554	4.561818
2.814875	239.530984	4.566822
2.645299	238.527506	4.571827
2.450285	236.789809	4.576832
2.462826	242.457309	4.581837
2.837608	236.067980	4.586842
2.729594	248.763044	4.591846
2.585253	249.123123	4.596851
2.717311	234.964610	4.601856
2.696901	242.659866	4.606861
2.714491	230.778626	4.611866
2.461710	228.111966	4.616870
2.869394	232.223354	4.621875
2.647428	224.699893	4.626880
2.520170	239.730251	4.631885
2.940566	235.438352	4.636890
2.656831	229.536562	4.641894
2.596413	230.790883	4.646899
2.903220	231.594064	4.651904
2.814866	238.772103	4.656909
2.705099	222.829867	4.661914
2.256908	228.844400	4.666918
2.688364	233.339420	4.671923
2.990647	240.040538	4.676928
2.829220	243.933393	4.681933
2.830600	231.704763	4.686938
2.775721	241.810461	4.691942
2.606168	249.393465	4.696947
2.495151	233.430113	4.701952
2.286395	242.295383	4.706957
2.127486	235.988312	4.711962
2.538956	244.899867	4.716966
2.721832	254.333938	4.721971
3.000967	258.745259	4.726976
2.773762	260.436674	4.731981
3.170589	259.603438	4.736986
2.932544	266.861137	4.741990
2.804303	265.180066	4.746995
3.055408	258.413575	4.752000
3.110503	267.943013	4.757005
3.346229	266.277645	4.762010
3.355454	269.943530	4.767014
2.552802	255.470515	4.772019
3.100059	253.116560	4.777024
3.097375	266.206037	4.782029
2.905399	255.393523	4.787034
2.994140	266.951925	4.792038
2.864140	268.255068	4.797043
2.791737	260.204009	4.802048
3.079520	269.395952	4.807053
3.223543	267.765503	4.812058
2.929180	269.025415	4.817062
3.261805	271.586339	4.822067
3.306903	263.370977	4.827072
3.085731	279.870307	4.832077
3.067838	271.297338	4.837082
3.239966	266.680483	4.842086
3.232833	262.242106	4.847091
3.515616	261.127606	4.852096
3.212724	271.797334	4.857101
3.300754	263.676293	4.862106
3.130460	273.021843	4.867110
3.403875	271.091526	4.872115
3.377756	266.360878	4.877120
3.069244	271.813768	4.882125
3.383404	275.847710	4.887130
3.667119	271.725647	4.892134
3.033667	273.592476	4.897139
3.401421	264.440010	4.902144
3.267323	272.269943	4.907149
3.294707	268.222297	4.912154
3.009161	274.963345	4.917158
2.908774	280.894257	4.922163
3.296705	273.741016	4.927168
2.809589	284.125126	4.932173
3.391076	288.346674	4.937178
3.764493	299.675621	4.942182
3.749083	300.751404	4.947187
3.844758	280.729685	4.952192
3.533220	283.741435	4.957197
3.232050	281.583224	4.962202
3.138543	287.944771	4.967206
3.714276	295.458849	4.972211
3.626173	297.144599	4.977216
3.672497	308.787412	4.982221
3.599831	299.220040	4.987226
3.489354	296.486982	4.992230
3.271454	300.684418	4.997235
3.787604	295.330959	5.002240
3.665272	303.853979	5.007245
3.636620	304.877687	5.012250
3.804754	299.926406	5.017254
3.782816	294.608375	5.022259
3.749914	298.556330	5.027264
3.720721	295.609318	5.032269
3.886232	286.011197	5.037274
3.343985	278.058060	5.042278
3.300366	289.304305	5.047283
3.867439	284.712031	5.052288
3.911945	296.873341	5.057293
3.687545	297.186293	5.062298
3.738318	289.633621	5.067302
3.756514	297.271203	5.072307
3.984219	300.415073	5.077312
3.756412	306.211001	5.082317
3.997483	302.833637	5.087322
3.937987	302.051690	5.092326
3.774250	302.099638	5.097331
3.809916	300.192111	5.102336
3.738517	295.090460	5.107341
3.933725	303.404804	5.112346
3.831973	299.907397	5.117350
3.466651	305.855351	5.122355
3.774948	297.057657	5.127360
3.280757	309.219578	5.132365
3.925046	304.188658	5.137370
3.875981	300.374088	5.142374
3.635687	303.055543	5.147379
3.873394	304.775946	5.152384
3.641245	305.015194	5.157389
3.777130	311.884796	5.162394
4.196555	316.732303	5.167398
4.193032	324.385533	5.172403
4.590941	311.699660	5.177408
4.104420	312.235791	5.182413
3.835768	292.419627	5.187418
3.917165	304.249229	5.192422
3.875839	311.062729	5.197427
4.189920	313.303494	5.202432
3.853426	332.731513	5.207437
4.390239	320.022632	5.212442
4.268947	331.759918	5.217446
4.132825	332.437140	5.222451
4.423486	328.330094	5.227456
3.948539	323.464772	5.232461
4.383376	317.414752	5.237466
4.221635	320.824399	5.242470
4.295180	319.642915	5.247475
4.083153	308.553268	5.252480
3.923401	320.445509	5.257485
4.297149	326.803503	5.262490
4.663909	331.615137	5.267494
4.478062	327.799135	5.272499
4.164653	309.695353	5.277504
3.852678	317.519835	5.282509
4.440930	327.144151	5.287514
4.312444	326.150834	5.292518
4.363698	334.792931	5.297523
4.550113	328.650249	5.302528
4.526393	334.333654	5.307533
4.347573	326.577244	5.312538
4.259326	319.541512	5.317542
4.138481	337.626273	5.322547
4.265553	323.361943	5.327552
4.003319	329.905370	5.332557
4.346869	327.411481	5.337562
4.389277	335.087697	5.342566
4.486164	331.431685	5.347571
4.420406	327.682428	5.352576
4.303244	331.564818	5.357581
4.643867	335.423104	5.362586
4.472207	335.659835	5.367590
4.141943	339.899371	5.372595
4.387084	326.844109	5.377600
4.337854	332.860698	5.382605
4.561531	333.806709	5.387610
4.634044	335.786342	5.392614
4.637385	328.249991	5.397619
4.698753	327.316996	5.402624
4.105175	338.697959	5.407629
4.593352	349.226286	5.412634
4.813289	354.243791	5.417638
4.744394	355.565634	5.422643
4.933266	362.624808	5.427648
5.202361	350.960341	5.432653
4.607230	340.102045	5.437658
4.646484	330.523225	5.442662
4.916752	329.533339	5.447667
4.903091	319.338124	5.452672
4.634643	323.799291	5.457677
4.901355	322.769540	5.462682
4.943360	324.989844	5.467686
4.719122	332.718897	5.472691
4.907623	328.843471	5.477696
4.987596	330.378057	5.482701
5.070706	327.158074	5.487706
4.574643	330.015287	5.492710
4.533566	337.090623	5.497715
4.584629	334.847043	5.502720
4.485674	339.243837	5.507725
4.961381	351.105270	5.512730
4.954530	348.793527	5.517734
4.471453	335.806944	5.522739
5.061621	349.876571	5.527744
5.098622	359.359332	5.532749
4.913043	352.582230	5.537754
5.157887	362.013013	5.542758
4.915827	356.828304	5.547763
4.978525	361.545058	5.552768
4.915889	353.064901	5.557773
5.164391	365.895796	5.562778
5.186742	358.935468	5.567782
4.887514	355.427531	5.572787
5.058297	350.295626	5.577792
5.118182	358.636355	5.582797
5.279024	352.920792	5.587802
5.133170	344.710761	5.592806
4.849577	337.312299	5.597811
4.935165	342.791912	5.602816
5.031096	360.703259	5.607821
4.981861	359.700763	5.612826
5.133007	358.137010	5.617830
5.021354	360.697714	5.622835
5.179217	360.135521	5.627840
4.887701	371.127264	5.632845
5.070319	368.821045	5.637850
5.317454	367.436958	5.642854
5.195707	369.643930	5.647859
5.266003	366.040463	5.652864
5.006522	363.621167	5.657869
5.247488	359.449524	5.662874
5.269729	363.832769	5.667878
4.995037	374.241753	5.672883
5.395587	359.791797	5.677888
5.395875	365.184309	5.682893
5.351399	365.594159	5.687898
5.582910	361.697986	5.692902
5.249007	363.463914	5.697907
5.597685	357.995293	5.702912
5.481629	368.822804	5.707917
5.130531	358.003612	5.712922
5.131671	360.508737	5.717926
5.323242	372.101892	5.722931
5.425094	364.434754	5.727936
5.348105	373.550999	5.732941
5.172389	363.964144	5.737946
5.442233	359.147557	5.742950
5.100044	364.528502	5.747955
5.914613	376.775089	5.752960
5.284833	379.771671	5.757965
5.122075	362.367110	5.762970
5.396719	374.228704	5.767974
5.452923	391.020063	5.772979
5.730324	385.610597	5.777984
5.312680	387.481959	5.782989
5.678999	398.074504	5.787994
5.738473	392.349072	5.792998
5.373389	397.929974	5.798003
5.629352	396.262228	5.803008
5.630175	393.500461	5.808013
5.852192	395.686625	5.813018
5.734607	389.989724	5.818022
5.762755	393.407411	5.823027
6.087952	392.540642	5.828032
5.701841	389.423605	5.833037
5.778104	382.210626	5.838042
5.576938	366.156686	5.843046
5.724198	387.088499	5.848051
5.800371	386.397157	5.853056
5.833610	391.360537	5.858061
5.594879	384.963613	5.863066
5.266825	378.506691	5.868070
5.541420	381.501126	5.873075
5.770832	379.826925	5.878080
6.006689	387.229198	5.883085
6.060859	387.942400	5.888090
5.872028	391.520340	5.893094
5.880754	395.942931	5.898099
6.103744	390.907746	5.903104
5.962584	400.493839	5.908109
5.768280	398.632472	5.913114
5.955996	388.284870	5.918118
5.882209	397.976826	5.923123
6.159930	388.252708	5.928128
5.981012	391.818942	5.933133
5.991905	391.682668	5.938138
6.201704	388.430248	5.943142
5.835879	390.661854	5.948147
5.975117	392.773515	5.953152
6.356940	393.608881	5.958157
5.663246	382.633081	5.963162
5.939788	386.191580	5.968166
5.778297	394.009533	5.973171
5.861332	388.988447	5.978176
5.877126	402.502413	5.983181
5.748159	394.891637	5.988186
5.828542	392.929925	5.993190
5.891144	400.666965	5.998195
6.119732	402.477100	6.003200
5.890257	395.785986	6.008205
5.631501	397.375880	6.013210
6.062681	396.235416	6.018214
5.841046	400.338183	6.023219
6.043612	406.768760	6.028224
6.359287	426.079035	6.033229
6.211456	411.603014	6.038234
6.275304	400.526030	6.043238
5.838924	400.126767	6.048243
6.064788	404.469200	6.053248
6.391033	415.746448	6.058253
6.041631	403.951500	6.063258
6.026561	394.294412	6.068262
6.173730	399.078494	6.073267
6.092934	383.943537	6.078272
5.816746	395.659752	6.083277
5.836843	418.619790	6.088282
6.356770	421.286677	6.093286
6.043437	429.884808	6.098291
6.406314	419.510154	6.103296
6.265199	414.657012	6.108301
6.171043	399.327704	6.113306
6.280546	400.508316	6.118310
6.069956	403.842005	6.123315
6.251052	388.836150	6.128320
6.220838	398.611864	6.133325
6.029730	392.226981	6.138330
6.044589	389.274038	6.143334
5.794205	397.338190	6.148339
6.195927	391.972468	6.153344
6.124192	396.320370	6.158349
6.251561	394.062566	6.163354
6.348864	395.205533	6.168358
6.141673	396.902726	6.173363
6.011310	393.321824	6.178368
5.904379	399.584800	6.183373
5.944298	399.856945	6.188378
6.199005	395.303537	6.193382
5.691965	400.737446	6.198387
6.218097	410.926226	6.203392
6.322025	412.890011	6.208397
5.921784	404.995386	6.213402
6.119467	401.261886	6.218406
6.269514	425.315967	6.223411
6.311490	417.680820	6.228416
5.962453	406.930123	6.233421
5.698207	412.047953	6.238426
6.589346	409.831015	6.243430
6.117547	408.809489	6.248435
5.907501	407.807570	6.253440
6.307666	408.314884	6.258445
5.903273	399.048265	6.263450
6.161571	402.465732	6.268454
5.854129	402.139445	6.273459
6.342726	408.207706	6.278464
5.834648	405.314121	6.283469
6.053023	421.960455	6.288474
6.228024	423.533582	6.293478
6.003198	426.403520	6.298483
6.317058	423.554784	6.303488
6.618686	420.400226	6.308493
5.920138	404.963001	6.313498
6.030407	393.167129	6.318502
5.973167	400.780155	6.323507
5.889398	390.788709	6.328512
5.976431	411.644094	6.333517
6.198846	422.488214	6.338522
6.503876	421.524141	6.343526
6.162371	416.923622	6.348531
6.209041	403.772495	6.353536
5.942387	397.210676	6.358541
5.866097	402.713170	6.363546
6.031811	401.112663	6.368550
6.176274	423.089104	6.373555
6.293493	421.199829	6.378560
6.273456	422.261783	6.383565
6.122927	409.317951	6.388570
6.195407	406.240020	6.393574
5.928765	397.743496	6.398579
6.201754	398.063085	6.403584
6.173064	388.923111	6.408589
6.179130	397.695668	6.413594
6.401966	390.979189	6.418598
6.195313	404.314697	6.423603
6.590907	391.629340	6.428608
6.300888	393.644148	6.433613
6.028880	391.042410	6.438618
6.265179	394.582908	6.443622
6.167231	396.813570	6.448627
6.295896	396.104063	6.453632
6.194497	401.968093	6.458637
6.284771	396.516990	6.463642
6.380723	391.085866	6.468646
5.853607	402.667218	6.473651
5.984739	402.050840	6.478656
5.818726	398.519058	6.483661
6.128498	401.544178	6.488666
6.122745	396.610413	6.493670
5.784704	402.729517	6.498675
6.142325	397.763009	6.503680
6.377885	398.269952	6.508685
5.989650	400.925798	6.513690
5.938352	393.468714	6.518694
5.829966	394.910569	6.523699
5.890927	398.427610	6.528704
5.904655	399.104688	6.533709
5.956653	404.385246	6.538714
6.253572	400.700041	6.543718
6.000869	398.546220	6.548723
5.922303	401.748523	6.553728
6.062757	398.184740	6.558733
6.016058	396.534355	6.563738
6.272413	402.256854	6.568742
5.950189	402.294539	6.573747
6.153633	396.536384	6.578752
6.308515	397.936420	6.583757
6.069785	401.755681	6.588762
6.090544	403.275807	6.593766
5.828208	402.625718	6.598771
6.128592	405.504390	6.603776
6.160470	421.472570	6.608781
6.168885	414.870325	6.613786
5.882302	413.277224	6.618790
5.773323	422.004119	6.623795
6.591864	432.068517	6.628800
6.659735	427.669770	6.633805
6.115816	414.573806	6.638810
6.082881	403.244270	6.643814
5.859362	397.748038	6.648819
6.321119	394.027644	6.653824
5.783003	402.796187	6.658829
5.381583	406.591673	6.663834
5.953028	424.443296	6.668838
5.888663	431.355979	6.673843
6.357811	427.295721	6.678848
6.485039	425.569763	6.683853
6.246374	435.037439	6.688858
6.705669	431.218381	6.693862
6.105111	424.742626	6.698867
5.708414	408.286877	6.703872
5.981444	421.635914	6.708877
6.390361	431.236711	6.713882
6.593240	419.630518	6.718886
6.045693	407.879824	6.723891
5.927656	401.909877	6.728896
6.052240	407.382267	6.733901
6.109011	406.710515	6.738906
6.333681	408.070579	6.743910
6.058523	402.577173	6.748915
6.307088	386.893343	6.753920
5.978547	399.375415	6.758925
6.031692	401.321954	6.763930
6.297282	381.877006	6.768934
6.152143	394.297328	6.773939
6.172620	392.093930	6.778944
6.234161	391.857308	6.783949
5.937313	400.387178	6.788954
6.217333	397.398415	6.793958
6.074016	402.268883	6.798963
6.483201	401.243952	6.803968
6.334508	392.545559	6.808973
5.883822	396.578705	6.813978
6.336304	393.817726	6.818982
6.356337	394.522769	6.823987
6.303789	396.622380	6.828992
6.042844	401.848590	6.833997
6.023100	399.591663	6.839002
6.211583	397.023193	6.844006
6.035020	396.382779	6.849011
6.272016	393.438240	6.854016
6.591748	393.827841	6.859021
5.766745	399.145875	6.864026
6.239510	396.629196	6.869030
5.954522	403.156293	6.874035
6.175580	399.770185	6.879040
6.071042	401.130298	6.884045
6.103810	408.085297	6.889050
6.451787	399.209341	6.894054
6.198496	407.845472	6.899059
6.638990	401.217071	6.904064
6.116830	389.001798	6.909069
5.818145	379.240326	6.914074
6.101515	383.309193	6.919078
6.283011	403.143883	6.924083
6.366408	392.144577	6.929088
5.945373	383.823998	6.934093
5.773175	385.513027	6.939098
6.294478	392.480858	6.944102
6.074589	395.534681	6.949107
6.116768	397.810221	6.954112
6.415062	397.789751	6.959117
6.004457	388.355048	6.964122
5.901197	380.753244	6.969126
5.851367	388.636376	6.974131
6.156249	397.153825	6.979136
6.259030	399.259092	6.984141
6.021390	407.813301	6.989146
6.294472	403.200803	6.994150
6.309882	399.094523	6.999155
5.919801	382.832083	7.004160
6.130198	375.162358	7.009165
6.001859	388.953364	7.014170
6.275578	393.594335	7.019174
5.951856	393.665421	7.024179
6.003344	396.845990	7.029184
6.236291	395.883593	7.034189
5.963146	400.754247	7.039194
6.557399	396.824639	7.044198
6.092444	390.223631	7.049203
5.942961	372.504277	7.054208
6.223059	386.959968	7.059213
6.547230	388.607849	7.064218
6.370378	384.253584	7.069222
6.120053	371.470563	7.074227
6.240879	371.780025	7.079232
6.163172	368.572259	7.084237
5.844618	370.073975	7.089242
6.182516	370.719474	7.094246
6.162883	375.640296	7.099251
6.006024	371.969263	7.104256
5.850375	374.768140	7.109261
5.849345	370.982303	7.114266
5.974000	366.447873	7.119270
5.674906	373.910701	7.124275
6.064520	388.806477	7.129280
6.326376	396.414219	7.134285
5.984528	403.511764	7.139290
6.090346	396.861428	7.144294
6.457142	398.112114	7.149299
5.864016	407.521645	7.154304
6.247859	401.463460	7.159309
6.084747	402.795580	7.164314
6.372347	394.390410	7.169318
6.034288	394.469000	7.174323
6.552595	386.498057	7.179328
6.056120	382.309597	7.184333
6.011045	380.112517	7.189338
6.152485	373.138777	7.194342
5.882868	369.469839	7.199347
5.940723	373.541118	7.204352
5.957092	377.240971	7.209357
6.270561	396.380088	7.214362
6.147572	385.459758	7.219366
6.090658	396.730385	7.224371
6.092858	397.629404	7.229376
5.921617	396.590275	7.234381
5.905212	404.922350	7.239386
6.397204	401.375736	7.244390
6.271652	397.851265	7.249395
6.174678	387.430430	7.254400
6.195364	379.161623	7.259405
5.891213	387.261512	7.264410
5.929428	384.365482	7.269414
5.665733	401.103657	7.274419
6.086869	396.340349	7.279424
6.470996	398.154130	7.284429
5.870850	393.931329	7.289434
6.302708	407.410937	7.294438
6.129428	407.544334	7.299443
6.115090	398.054465	7.304448
6.442946	405.933674	7.309453
6.303147	393.019060	7.314458
6.065577	379.753205	7.319462
5.984386	381.185228	7.324467
6.080700	388.936018	7.329472
6.045686	379.798084	7.334477
6.032691	397.652522	7.339482
6.557604	396.915880	7.344486
6.185912	379.296660	7.349491
5.988131	371.207103	7.354496
5.824984	367.803913	7.359501
5.594048	383.445170	7.364506
6.299225	386.444081	7.369510
5.714418	399.855426	7.374515
6.147508	402.526428	7.379520
6.072879	404.872225	7.384525
6.129681	406.387567	7.389530
6.300649	391.716690	7.394534
6.346822	401.353461	7.399539
6.420524	395.466025	7.404544
6.318961	390.081027	7.409549
5.900310	401.140811	7.414554
6.102744	391.166107	7.419558
6.338112	387.493860	7.424563
6.163545	386.064553	7.429568
6.090895	366.572032	7.434573
6.021211	360.787288	7.439578
6.188211	367.137698	7.444582
6.172938	373.755100	7.449587
6.310344	361.716769	7.454592
6.152141	366.788805	7.459597
5.994020	373.013083	7.464602
6.244548	360.740725	7.469606
6.187771	366.375940	7.474611
5.993496	364.470369	7.479616
5.870590	365.878513	7.484621
5.693560	373.290540	7.489626
6.023855	394.397877	7.494630
6.181557	400.147960	7.499635
6.199281	392.853500	7.504640
6.569640	388.386123	7.509645
6.145708	387.008174	7.514650
6.245419	372.048767	7.519654
6.036086	369.967690	7.524659
6.100391	365.862005	7.529664
6.184065	370.410709	7.534669
5.757504	374.615682	7.539674
6.015290	366.674866	7.544678
6.261009	379.251865	7.549683
6.016032	381.359856	7.554688
6.153435	382.418036	7.559693
6.110870	380.889712	7.564698
6.391699	380.188753	7.569702
6.021128	378.753029	7.574707
5.688788	368.571282	7.579712
6.042607	382.457084	7.584717
6.007240	398.123792	7.589722
6.082002	401.485611	7.594726
6.251621	408.977798	7.599731
6.226596	404.823351	7.604736
6.322514	398.165380	7.609741
5.964068	389.856338	7.614746
6.057430	388.347538	7.619750
6.317003	402.607726	7.624755
6.175639	394.619522	7.629760
5.909311	384.690279	7.634765
6.041856	400.454099	7.639770
6.316051	386.812420	7.644774
6.210485	389.090520	7.649779
6.112300	374.118296	7.654784
6.299701	370.315070	7.659789
5.962393	378.516746	7.664794
5.949161	364.157801	7.669798
5.941638	381.705639	7.674803
6.167327	392.698581	7.679808
6.241516	396.610080	7.684813
5.934340	395.560901	7.689818
6.172218	396.388726	7.694822
6.294631	407.705641	7.699827
6.241853	397.063370	7.704832
6.081455	381.510019	7.709837
5.828001	383.050094	7.714842
6.053619	392.553344	7.719846
5.962014	404.015416	7.724851
6.107924	404.959114	7.729856
6.170539	402.775772	7.734861
6.343494	403.297029	7.739866
6.344697	388.781550	7.744870
5.869407	372.933827	7.749875
6.069682	379.321554	7.754880
6.506259	378.945869	7.759885
5.962511	374.852462	7.764890
6.005298	369.183083	7.769894
6.208156	372.934344	7.774899
6.322949	368.334650	7.779904
5.896850	363.854717	7.784909
5.701178	372.689083	7.789914
6.245590	386.156743	7.794918
6.311217	400.485552	7.799923
6.163073	380.736938	7.804928
6.178167	373.595464	7.809933
6.213665	362.363161	7.814938
6.176502	365.423622	7.819942
6.050626	372.609318	7.824947
6.071310	364.023398	7.829952
5.906565	363.998498	7.834957
5.862241	372.479432	7.839962
6.512491	382.380840	7.844966
6.078114	386.930084	7.849971
6.136482	375.854223	7.854976
5.909826	372.237174	7.859981
5.932250	379.855942	7.864986
6.405717	382.981235	7.869990
6.074778	383.130872	7.874995
6.094722	378.540566	7.880000
6.062031	374.505010	7.885005
6.101007	384.507839	7.890010
6.109948	378.068129	7.895014
6.020358	384.241991	7.900019
6.081298	393.536890	7.905024
6.317642	397.008707	7.910029
5.938101	403.416680	7.915034
6.463363	388.100847	7.920038
6.095037	384.223089	7.925043
5.592968	388.192121	7.930048
6.013952	391.003261	7.935053
6.340280	400.558119	7.940058
6.489189	394.084174	7.945062
6.133675	387.397950	7.950067
5.884970	383.978336	7.955072
5.741354	381.638124	7.960077
5.759333	401.101069	7.965082
6.131088	403.138905	7.970086
6.083204	405.838245	7.975091
6.271737	404.151077	7.980096
5.950410	408.577018	7.985101
5.965435	410.161834	7.990106
6.421618	402.433438	7.995110
6.282251	403.554619	8.000115
6.038716	403.601584	8.005133
6.229326	403.465024	8.010150
5.939823	403.271365	8.015168
6.140809	397.605183	8.020186
5.840259	408.098326	8.025203
6.022085	402.158369	8.030221
6.421816	406.556698	8.035238
6.231398	403.390567	8.040256
6.534612	407.510218	8.045274
5.901858	411.391188	8.050291
6.146266	405.229664	8.055309
6.310277	405.897248	8.060326
5.936135	411.633275	8.065344
6.195291	407.654174	8.070362
6.171297	396.635520	8.075379
6.180017	405.487222	8.080397
6.391497	403.668797	8.085414
6.368689	408.054031	8.090432
6.297159	409.814670	8.095450
6.269315	402.080641	8.100467
6.179036	406.768560	8.105485
6.509538	407.443808	8.110502
6.103137	399.945485	8.115520
6.047331	392.216485	8.120538
6.091072	403.110450	8.125555
6.007841	401.258353	8.130573
6.309502	401.677768	8.135590
6.020411	407.867980	8.140608
6.128390	408.386391	8.145626
6.508804	409.246469	8.150643
6.260593	404.779579	8.155661
6.346113	404.608261	8.160678
6.208488	407.135099	8.165696
6.420952	402.552361	8.170714
6.312795	411.075613	8.175731
6.222715	411.956717	8.180749
6.236344	393.941840	8.185766
6.104981	410.549782	8.190784
6.126569	402.453659	8.195802
6.265919	404.811609	8.200819
6.362952	401.530956	8.205837
6.395393	401.198558	8.210854
6.006286	406.992963	8.215872
6.222691	405.675848	8.220890
6.361816	409.968328	8.225907
6.114995	410.720281	8.230925
6.189519	405.869856	8.235942
5.992069	410.491278	8.240960
6.159062	403.773720	8.245978
6.151890	410.267221	8.250995
6.017314	417.093215	8.256013
6.780481	419.324248	8.261030
6.233368	435.187937	8.266048
6.501109	442.408309	8.271066
6.507843	435.157870	8.276083
6.434383	423.598022	8.281101
6.198273	407.484377	8.286118
6.478355	425.628997	8.291136
6.821237	422.519226	8.296154
6.611173	420.451534	8.301171
6.455944	414.614036	8.306189
6.686545	409.306894	8.311206
6.554924	409.106577	8.316224
6.278309	410.725599	8.321242
6.563026	412.609909	8.326259
6.234361	415.374863	8.331277
6.287042	401.893506	8.336294
6.123764	407.296409	8.341312
6.505162	406.346823	8.346330
6.224039	410.019381	8.351347
5.715689	420.663469	8.356365
6.272444	423.487891	8.361382
6.467226	434.867063	8.366400
6.565578	442.328853	8.371418
6.569311	437.076591	8.376435
6.677036	444.033523	8.381453
6.778201	446.597394	8.386470
6.602260	440.925705	8.391488
6.556205	437.531150	8.396506
6.842553	438.856968	8.401523
6.298394	437.502618	8.406541
6.664621	434.377562	8.411558
6.480626	437.086676	8.416576
6.515064	436.275638	8.421594
6.757734	439.757341	8.426611
6.437584	439.812438	8.431629
6.671098	437.098107	8.436646
6.624729	444.374628	8.441664
6.537163	427.749984	8.446682
6.415333	432.144930	8.451699
6.509856	437.762615	8.456717
6.938081	430.207165	8.461734
6.574894	427.623335	8.466752
6.260615	425.473499	8.471770
6.770845	431.265631	8.476787
6.601457	439.873835	8.481805
6.742666	436.229587	8.486822
6.527507	438.061450	8.491840
6.829058	434.188502	8.496858
6.746382	432.452049	8.501875
6.262638	430.019471	8.506893
6.562035	429.727900	8.511910
7.003332	442.181129	8.516928
6.638503	435.714603	8.521946
6.574720	426.056743	8.526963
6.514028	443.566923	8.531981
6.786400	433.896303	8.536998
6.638632	445.420585	8.542016
6.686531	438.547944	8.547034
7.047645	438.392992	8.552051
6.579889	431.164438	8.557069
6.527862	427.583291	8.562087
6.597480	433.033261	8.567104
6.582278	442.774703	8.572122
6.800082	435.515885	8.577139
6.910957	439.292816	8.582157
6.823871	430.541301	8.587175
6.699980	435.829236	8.592192
6.478032	438.071837	8.597210
6.641639	435.211221	8.602227
6.497476	440.636362	8.607245
6.911891	446.040264	8.612263
6.712815	444.843123	8.617280
6.768955	437.907509	8.622298
7.061103	430.126186	8.627315
6.655141	440.116177	8.632333
6.842583	436.498719	8.637351
6.874439	430.044651	8.642368
6.810608	443.073615	8.647386
6.778735	435.710877	8.652403
6.969155	442.232100	8.657421
6.587213	440.672948	8.662439
6.665015	438.818786	8.667456
6.581230	445.132877	8.672474
6.944719	444.246683	8.677491
6.371266	442.364350	8.682509
6.494519	436.622844	8.687527
6.535190	436.561306	8.692544
6.598477	450.648866	8.697562
6.528972	440.739995	8.702579
6.525583	442.140168	8.707597
7.061282	451.389831	8.712615
7.002926	458.352619	8.717632
6.952066	461.602050	8.722650
7.203204	450.661608	8.727667
6.840759	446.953722	8.732685
7.144563	439.668852	8.737703
6.988965	437.892509	8.742720
6.629551	437.555713	8.747738
7.169948	432.043338	8.752755
6.836603	430.111011	8.757773
7.152255	438.638700	8.762791
7.249665	434.787154	8.767808
7.158117	434.707160	8.772826
7.167210	428.341698	8.777843
6.930440	436.160333	8.782861
7.070704	435.223512	8.787879
7.295274	434.596721	8.792896
6.981001	442.944689	8.797914
7.205507	429.355334	8.802931
7.179265	442.128682	8.807949
7.171879	434.294406	8.812967
7.078684	434.798497	8.817984
6.831742	442.740465	8.823002
6.909026	431.159585	8.828019
6.879523	441.547833	8.833037
6.769009	444.722696	8.838055
7.049420	445.487336	8.843072
6.950413	439.827119	8.848090
7.308288	438.209825	8.853107
7.080978	440.613144	8.858125
7.086294	439.652412	8.863143
7.344388	440.150888	8.868160
6.985623	441.696713	8.873178
7.606844	424.251805	8.878195
7.181185	430.002275	8.883213
6.998314	410.303516	8.888231
6.924131	410.670217	8.893248
6.862889	432.516549	8.898266
7.277547	428.316825	8.903283
7.094625	433.859004	8.908301
6.893452	438.705245	8.913319
7.161439	434.406589	8.918336
7.139283	440.987617	8.923354
7.337862	442.155542	8.928371
7.086500	438.956586	8.933389
7.240125	432.109744	8.938407
7.174765	434.077221	8.943424
6.970750	437.496485	8.948442
7.195819	434.838076	8.953459
7.176525	439.949846	8.958477
7.214584	445.120620	8.963495
7.428907	432.308479	8.968512
7.055597	433.275851	8.973530
7.220916	438.334218	8.978547
7.119614	431.373697	8.983565
6.744305	432.822859	8.988583
7.131919	434.561008	8.993600
7.178012	443.802772	8.998618
6.854241	442.653837	9.003635
7.125129	438.419655	9.008653
7.128371	439.326839	9.013671
7.215120	445.257600	9.018688
6.973482	446.118136	9.023706
7.082229	449.615326	9.028723
7.176183	436.985109	9.033741
7.148595	443.197578	9.038759
7.050697	442.545451	9.043776
7.081710	434.821146	9.048794
7.419535	438.420350	9.053811
7.115322	433.436978	9.058829
6.592216	439.998802	9.063847
7.216832	452.446288	9.068864
7.172492	463.653480	9.073882
7.323194	469.199082	9.078899
7.261977	466.163107	9.083917
7.319158	469.116520	9.088935
7.345339	462.660426	9.093952
7.162121	467.059052	9.098970
7.268541	469.304364	9.103987
7.319711	471.171453	9.109005
7.308270	465.340832	9.114023
7.349951	464.385297	9.119040
7.115522	470.568647	9.124058
7.383906	465.985883	9.129075
7.013810	473.233156	9.134093
7.423180	472.905461	9.139111
7.521507	469.576551	9.144128
7.138808	475.215010	9.149146
7.140505	466.041126	9.154163
7.312394	471.017122	9.159181
7.153061	477.129580	9.164199
7.486562	471.672907	9.169216
7.000434	476.671850	9.174234
7.418366	489.172093	9.179251
7.784524	502.398388	9.184269
7.761812	483.703845	9.189287
7.723023	473.760734	9.194304
7.411202	472.341925	9.199322
7.907097	468.963124	9.204339
7.648649	465.668099	9.209357
7.600908	464.192373	9.214375
7.364153	459.882809	9.219392
7.477807	468.368182	9.224410
7.826810	473.825441	9.229427
7.337747	465.431590	9.234445
7.327056	469.294993	9.239463
7.661697	474.532404	9.244480
7.311321	474.833826	9.249498
7.587071	466.736327	9.254515
7.906463	463.546192	9.259533
7.568773	472.336996	9.264551
7.664593	472.169876	9.269568
7.583495	469.634006	9.274586
7.616159	464.185422	9.279603
7.221884	463.791017	9.284621
7.092098	469.092341	9.289639
7.348632	463.035273	9.294656
7.234000	467.352074	9.299674
7.517532	469.761351	9.304691
7.562697	489.008645	9.309709
7.217567	493.783866	9.314727
7.993821	493.394631	9.319744
8.021645	502.286922	9.324762
7.596849	485.705462	9.329779
7.668288	465.144505	9.334797
7.788669	466.941476	9.339815
7.534284	461.314853	9.344832
7.425441	463.548964	9.349850
7.628957	488.770959	9.354867
7.710846	497.925337	9.359885
7.551039	499.977158	9.364903
7.947471	494.727954	9.369920
7.829612	497.563911	9.374938
7.576030	469.060118	9.379955
7.687690	471.010884	9.384973
7.570314	476.938651	9.389991
8.087165	484.808488	9.395008
7.857854	476.545227	9.400026
7.631004	468.694918	9.405043
7.730341	461.606481	9.410061
7.243718	469.584805	9.415079
7.789869	477.334638	9.420096
7.905431	495.670744	9.425114
7.463530	492.902118	9.430131
7.674746	486.390966	9.435149
7.992218	495.665375	9.440167
7.625649	493.744644	9.445184
7.766543	492.491006	9.450202
7.674814	502.558717	9.455219
7.984681	495.963317	9.460237
7.705576	500.078246	9.465255
8.035058	491.475022	9.470272
7.587302	498.851497	9.475290
7.801900	497.727179	9.480307
7.891548	497.354994	9.485325
7.856848	501.283793	9.490343
7.556702	488.545578	9.495360
7.672393	501.907435	9.500378
7.652685	495.542187	9.505395
7.695772	492.775725	9.510413
7.706994	505.162831	9.515431
7.755860	498.417947	9.520448
7.632793	503.412483	9.525466
7.544800	498.263768	9.530483
7.852751	498.711277	9.535501
7.659026	505.969120	9.540519
7.526921	514.464507	9.545536
7.877795	520.908212	9.550554
7.868069	524.263632	9.555571
8.302106	522.556951	9.560589
7.942800	519.186496	9.565607
8.104390	519.702529	9.570624
8.029289	522.413900	9.575642
8.258124	520.104238	9.580659
8.300875	503.512654	9.585677
7.937803	495.655363	9.590695
7.897368	492.665544	9.595712
7.809069	494.987982	9.600730
7.761740	502.125723	9.605747
8.119457	501.067462	9.610765
7.736674	503.328045	9.615783
8.014166	509.474668	9.620800
8.048210	523.276016	9.625818
8.028663	528.771492	9.630835
8.426869	528.480091	9.635853
8.112660	515.706193	9.640871
8.355668	511.035105	9.645888
8.155707	503.850158	9.650906
7.841782	500.203118	9.655923
8.054409	501.746056	9.660941
8.062298	499.754262	9.665959
7.981201	501.038184	9.670976
7.834079	503.300094	9.675994
7.817811	515.613617	9.681011
8.164698	519.816610	9.686029
8.314687	523.895724	9.691047
8.322206	523.101146	9.696064
8.334550	524.869167	9.701082
7.870186	515.681688	9.706099
8.032137	514.059038	9.711117
7.859101	525.962143	9.716135
7.962957	521.581397	9.721152
7.779026	521.961549	9.726170
8.245048	526.898109	9.731187
8.626235	517.674936	9.736205
8.478342	533.845622	9.741223
8.458516	528.614748	9.746240
8.541858	522.190892	9.751258
7.827439	516.653418	9.756275
8.039096	509.474122	9.761293
8.137450	515.659860	9.766311
8.488985	523.015792	9.771328
8.428234	530.102426	9.776346
8.014651	527.745018	9.781363
8.441794	518.648280	9.786381
8.082409	520.812084	9.791399
8.565872	525.124343	9.796416
8.182482	509.827837	9.801434
8.104306	507.322969	9.806451
8.541926	521.529697	9.811469
8.246413	516.422032	9.816487
8.135756	499.746415	9.821504
8.717972	514.332312	9.826522
8.198545	513.400206	9.831539
7.885658	496.076240	9.836557
8.195645	517.649030	9.841575
8.590452	520.914628	9.846592
8.916193	521.486741	9.851610
8.341833	515.554842	9.856627
8.423503	502.744335	9.861645
8.161157	508.859494	9.866663
8.285859	494.872662	9.871680
8.191044	511.209325	9.876698
8.192958	522.728759	9.881715
8.459237	521.339207	9.886733
8.495795	530.694405	9.891751
8.118484	524.981035	9.896768
8.367111	525.809994	9.901786
8.267854	528.171651	9.906803
8.464132	532.191138	9.911821
8.265706	529.050715	9.916839
8.183790	533.169218	9.921856
8.501069	528.085263	9.926874
8.057618	530.530096	9.931891
8.516645	523.450765	9.936909
8.263740	536.602054	9.941927
8.171151	533.002010	9.946944
8.457968	533.620133	9.951962
8.415227	543.362262	9.956979
8.569295	533.297027	9.961997
8.271166	531.834805	9.967015
8.462078	527.420943	9.972032
8.437631	535.243246	9.977050
8.286999	547.919768	9.982067
8.594736	553.153000	9.987085
8.590573	559.228181	9.992103
8.614824	567.163884	9.997120
8.964431	547.182696	10.002138
8.549394	548.299888	10.007155
8.563248	535.996612	10.012173
8.446812	536.356927	10.017191
8.338124	541.222332	10.022208
8.379254	550.977346	10.027226
8.443854	560.208438	10.032243
8.888326	557.346170	10.037261
8.809619	570.298575	10.042279
8.585717	564.987514	10.047296
8.874647	555.078857	10.052314
8.875353	558.236900	10.057331
8.822255	534.298286	10.062349
8.453794	536.515166	10.067367
8.220396	527.754558	10.072384
8.489444	550.518341	10.077402
8.507980	556.601375	10.082419
8.786904	551.660960	10.087437
8.847257	559.365500	10.092455
8.845874	557.725013	10.097472
8.793361	561.886091	10.102490
8.739007	562.783333	10.107507
8.837662	558.641020	10.112525
8.830635	564.595229	10.117543
8.698208	560.517951	10.122560
9.143463	562.203267	10.127578
8.884957	551.668975	10.132595
8.792411	533.669549	10.137613
8.850491	534.942630	10.142631
8.679643	528.877377	10.147648
8.818847	521.903365	10.152666
8.676640	528.821413	10.157683
8.679549	527.685891	10.162701
8.808281	535.623763	10.167719
8.806091	553.680836	10.172736
9.112527	553.241258	10.177754
8.681284	545.151349	10.182771
9.156610	536.630439	10.187789
9.110177	532.853079	10.192807
8.895131	529.093011	10.197824
8.855475	521.418946	10.202842
9.045905	530.158155	10.207859
8.974039	522.552213	10.212877
8.740445	525.873449	10.217895
8.819509	528.480164	10.222912
9.064020	525.990949	10.227930
8.735942	522.762556	10.232947
8.754993	528.065235	10.237965
8.666311	528.101095	10.242983
8.729631	537.360927	10.248000
9.013758	550.020966	10.253018
8.625624	569.303892	10.258035
8.628438	561.940075	10.263053
9.135337	559.094238	10.268071
8.921085	560.502176	10.273088
8.880911	558.390586	10.278106
8.989331	563.340314	10.283123
9.018027	564.541891	10.288141
9.270221	563.790254	10.293159
9.236418	567.951779	10.298176
9.371395	559.102006	10.303194
9.399228	559.380562	10.308211
8.978086	548.089006	10.313229
8.912140	534.379163	10.318247
8.773847	550.656340	10.323264
9.309021	549.562786	10.328282
8.884574	559.523043	10.333299
9.172243	566.815562	10.338317
9.164676	562.759336	10.343335
9.211075	569.628062	10.348352
9.243951	557.487749	10.353370
9.266906	561.653455	10.358387
9.326856	540.981709	10.363405
9.034573	532.889464	10.368423
8.729911	530.494533	10.373440
9.131049	543.283212	10.378458
9.197079	557.356046	10.383475
8.984733	551.415560	10.388493
9.271519	564.824331	10.393511
9.206246	559.651362	10.398528
8.958087	553.505994	10.403546
8.921421	552.768138	10.408563
9.176283	551.796980	10.413581
9.200226	553.191062	10.418599
9.123984	557.948941	10.423616
9.307066	551.066857	10.428634
9.203672	560.651532	10.433651
9.112632	560.118728	10.438669
9.249439	559.007681	10.443687
9.110048	554.013905	10.448704
9.578055	554.355586	10.453722
9.017563	564.037804	10.458739
9.088889	554.160851	10.463757
9.528848	553.360406	10.468775
9.199276	561.631449	10.473792
9.036360	556.925406	10.478810
9.169545	560.347320	10.483827
9.259987	554.632068	10.488845
9.299662	556.080235	10.493863
9.327886	556.723071	10.498880
9.473914	556.929302	10.503898
9.410115	558.760917	10.508915
9.599069	554.448545	10.513933
9.722220	554.598333	10.518951
9.350553	567.403788	10.523968
9.736445	552.966398	10.528986
9.651170	556.120964	10.534003
9.581658	555.777495	10.539021
9.682202	557.054767	10.544039
9.506974	559.216622	10.549056
9.405770	544.778604	10.554074
9.424786	556.825115	10.559091
9.403661	558.021164	10.564109
9.514277	553.911515	10.569127
9.426172	559.442367	10.574144
9.243635	550.383187	10.579162
9.567837	556.154404	10.584179
9.364971	566.109860	10.589197
9.739706	558.703157	10.594215
9.574726	558.079455	10.599232
9.424327	555.111376	10.604250
9.329302	559.343269	10.609267
9.222727	561.324870	10.614285
9.387061	558.639689	10.619303
9.349309	563.689010	10.624320
9.469612	560.828062	10.629338
9.642245	557.353963	10.634355
9.467971	565.716017	10.639373
9.371454	556.918554	10.644391
9.175705	560.232743	10.649408
9.398206	563.698918	10.654426
9.657142	565.793801	10.659443
9.706505	561.481709	10.664461
9.456624	552.847430	10.669479
9.295237	570.351791	10.674496
9.646563	570.063035	10.679514
9.888985	582.846141	10.684531
9.764635	588.825496	10.689549
9.665189	567.583496	10.694567
9.571394	581.736357	10.699584
10.063163	585.891167	10.704602
10.064776	573.977656	10.709619
9.559134	561.072636	10.714637
9.711783	557.938241	10.719655
9.832354	566.774859	10.724672
9.688434	558.131692	10.729690
9.635242	562.047034	10.734707
9.625440	559.465093	10.739725
9.764213	557.605347	10.744743
9.897780	569.686046	10.749760
9.424862	556.252419	10.754778
9.794019	563.031280	10.759795
9.762444	578.468234	10.764813
10.012721	573.615620	10.769831
9.723866	581.351228	10.774848
9.916176	572.272874	10.779866
9.876601	575.942675	10.784883
9.550866	580.947175	10.789901
10.081791	572.917792	10.794919
9.819995	584.566367	10.799936
9.924649	587.578079	10.804954
10.020885	582.960405	10.809971
10.003042	567.079330	10.814989
10.020386	559.043666	10.820007
9.593059	559.349958	10.825024
9.818617	566.148466	10.830042
9.908723	561.262345	10.835059
9.728417	577.807315	10.840077
10.101180	574.344755	10.845095
9.748494	582.916664	10.850112
9.820489	583.173145	10.855130
10.162244	585.922381	10.860147
9.908982	577.951398	10.865165
10.158629	576.600617	10.870183
9.918018	584.180805	10.875200
9.922531	582.206882	10.880218
9.956426	564.382925	10.885235
9.928291	580.979074	10.890253
10.106985	565.137892	10.895271
9.757879	578.159684	10.900288
9.994981	574.794977	10.905306
9.907961	577.089068	10.910323
9.756450	577.399291	10.915341
9.780615	573.360445	10.920359
9.827799	580.951633	10.925376
9.762014	579.739102	10.930394
9.730354	582.564147	10.935411
9.814514	586.367585	10.940429
10.239879	599.083011	10.945447
10.184289	612.683745	10.950464
10.289878	609.502017	10.955482
10.123972	597.857157	10.960499
10.031518	598.829406	10.965517
9.923712	605.860287	10.970535
10.152113	616.635641	10.975552
9.938729	611.311208	10.980570
10.024983	607.164243	10.985587
10.157098	617.304207	10.990605
10.197670	605.288755	10.995623
10.294076	617.614604	11.000640
10.136845	614.166575	11.005658
10.358321	612.500595	11.010675
9.945433	609.401967	11.015693
9.852703	614.932818	11.020711
9.957012	612.735489	11.025728
9.913850	610.053165	11.030746
10.111819	602.912703	11.035763
9.869268	618.210432	11.040781
10.507981	627.152807	11.045799
10.407033	632.075419	11.050816
10.588564	624.360740	11.055834
10.460426	609.641314	11.060851
10.656583	613.209888	11.065869
10.680768	603.727494	11.070887
10.590115	615.346965	11.075904
10.380628	611.444431	11.080922
10.272936	608.110829	11.085939
10.207347	615.837827	11.090957
10.354655	608.691777	11.095975
10.425904	607.531941	11.100992
10.540682	613.042602	11.106010
10.323781	601.261311	11.111027
10.259568	620.282211	11.116045
10.451460	610.564182	11.121063
10.609754	605.884260	11.126080
10.536948	610.212678	11.131098
10.517650	615.330806	11.136115
10.511224	608.590896	11.141133
10.389178	607.893748	11.146151
10.572494	620.088680	11.151168
10.588398	611.366265	11.156186
10.670316	608.374665	11.161203
10.098791	611.517248	11.166221
10.481098	608.885328	11.171239
10.475285	612.683593	11.176256
10.309965	614.802479	11.181274
10.294803	612.061191	11.186291
10.194430	624.394436	11.191309
10.617893	631.709969	11.196327
10.790464	635.659200	11.201344
10.360963	637.345686	11.206362
11.078812	629.591599	11.211379
10.455921	627.742230	11.216397
10.820468	618.255039	11.221415
10.654156	607.226339	11.226432
10.386319	620.380762	11.231450
10.736735	609.053518	11.236467
10.557743	620.738602	11.241485
10.930558	623.571476	11.246503
10.960919	625.117248	11.251520
10.725659	612.163869	11.256538
10.714722	610.665500	11.261555
10.430159	610.621796	11.266573
10.640416	611.620686	11.271591
10.575642	614.290995	11.276608
10.713131	638.267361	11.281626
11.251061	634.281800	11.286643
10.800908	622.344052	11.291661
10.518467	612.076656	11.296679
10.622536	616.613369	11.301696
10.743892	637.639648	11.306714
11.156371	626.562136	11.311731
10.643265	629.421248	11.316749
10.855605	622.167972	11.321767
11.278299	623.962536	11.326784
10.600357	623.980035	11.331802
10.787013	609.454136	11.336819
10.760815	612.285172	11.341837
10.711976	617.886703	11.346855
10.767268	613.192144	11.351872
10.774591	627.982985	11.356890
11.097984	631.799965	11.361907
11.110399	639.830966	11.366925
11.071976	627.101853	11.371943
10.943054	619.304538	11.376960
10.774619	624.550310	11.381978
10.996954	614.574695	11.386995
10.554237	635.329047	11.392013
10.746245	628.939315	11.397031
10.807354	635.498764	11.402048
10.704160	638.727175	11.407066
11.083842	632.747478	11.412083
10.896842	640.640253	11.417101
11.061954	630.090874	11.422119
11.132426	628.197551	11.427136
10.826982	631.758645	11.432154
10.942059	623.758532	11.437171
11.102609	634.135121	11.442189
11.164682	638.278230	11.447207
11.345519	632.570814	11.452224
10.881956	638.402828	11.457242
11.056975	633.228232	11.462259
10.816950	635.459288	11.467277
10.805058	630.629008	11.472295
11.246968	640.258465	11.477312
10.842530	645.695677	11.482330
11.183287	636.261623	11.487347
11.337868	638.483632	11.492365
11.224794	635.658954	11.497383
11.210617	633.653278	11.502400
11.017145	630.647831	11.507418
10.998920	639.554716	11.512435
10.605618	638.631832	11.517453
11.026337	655.840304	11.522471
11.669651	659.411610	11.527488
11.405044	663.847783	11.532506
11.278542	644.100418	11.537523
11.558028	641.500873	11.542541
11.221721	643.088074	11.547559
11.617168	635.203526	11.552576
11.132178	637.505459	11.557594
10.963812	630.224873	11.562611
11.408375	632.648846	11.567629
11.442163	638.557154	11.572647
11.355086	630.426154	11.577664
10.999484	637.996869	11.582682
11.333385	633.536859	11.587699
11.296981	642.912867	11.592717
11.179980	652.408913	11.597735
11.510023	663.349740	11.602752
11.207335	678.661620	11.607770
11.592264	678.750345	11.612787
11.422571	671.249107	11.617805
11.361685	673.760722	11.622823
11.566771	670.810128	11.627840
11.367863	677.632913	11.632858
11.300894	667.065251	11.637875
11.424191	674.322445	11.642893
11.790137	670.045295	11.647911
11.876899	667.042254	11.652928
11.561335	661.408366	11.657946
11.359140	633.395335	11.662963
11.617455	639.938862	11.667981
11.547784	646.523711	11.672999
11.238344	639.258214	11.678016
11.190020	649.493231	11.683034
11.526044	659.336285	11.688051
11.262754	669.741155	11.693069
11.214274	672.249534	11.698087
11.442825	659.229155	11.703104
11.446592	673.037618	11.708122
11.589807	668.589884	11.713139
11.790156	667.721048	11.718157
11.481736	663.686270	11.723175
11.767271	664.663053	11.728192
11.542943	667.635169	11.733210
11.697895	669.931919	11.738227
11.213138	667.102644	11.743245
11.086703	667.640985	11.748263
11.319701	674.000541	11.753280
11.671979	690.112974	11.758298
11.684237	698.383781	11.763315
11.811560	692.533245	11.768333
11.783915	695.008652	11.773351
11.949167	689.663223	11.778368
11.710609	692.854222	11.783386
11.876628	700.680303	11.788403
11.569985	695.227199	11.793421
11.896057	689.252027	11.798439
11.858762	688.828421	11.803456
12.048704	695.445888	11.808474
11.599039	689.773570	11.813491
11.941054	680.347549	11.818509
11.937473	692.230201	11.823527
12.207549	686.370201	11.828544
11.659346	683.791966	11.833562
11.704712	672.158519	11.838579
11.937513	675.633249	11.843597
11.839339	688.137430	11.848615
12.125951	677.608842	11.853632
11.744580	681.537222	11.858650
11.938871	685.387994	11.863667
12.116656	693.542811	11.868685
11.938532	680.659042	11.873703
12.200432	674.126821	11.878720
12.064711	667.709261	11.883738
11.927832	657.950769	11.888755
11.984242	666.215035	11.893773
11.582018	662.879999	11.898791
11.770819	681.100070	11.903808
11.832660	698.018432	11.908826
11.922447	692.660697	11.913843
12.368444	691.322861	11.918861
12.172928	692.050191	11.923879
12.491759	689.085483	11.928896
12.089201	700.269688	11.933914
12.076329	691.509475	11.938931
12.105702	691.048060	11.943949
12.068236	700.122329	11.948967
12.406383	694.327822	11.953984
12.123116	678.300242	11.959002
12.010273	674.168906	11.964019
12.207794	677.266826	11.969037
12.024246	688.208470	11.974055
12.436043	687.407369	11.979072
12.303910	676.189901	11.984090
11.946142	670.477177	11.989107
12.002080	670.219225	11.994125
12.272448	683.983946	11.999143
12.411760	679.399068	12.004160
12.360025	694.802864	12.009178
12.337897	687.643695	12.014195
12.431745	683.141538	12.019213
12.107695	679.216424	12.024231
12.446477	683.927073	12.029248
12.163684	682.152867	12.034266
12.115072	692.187185	12.039283
12.247557	682.657678	12.044301
12.147107	697.971912	12.049319
12.623794	697.597834	12.054336
12.365889	697.610735	12.059354
12.203286	690.833859	12.064371
12.526642	696.619835	12.069389
12.147220	701.099832	12.074407
12.162458	690.838993	12.079424
12.035301	688.646913	12.084442
12.252639	687.838251	12.089459
12.435580	686.270764	12.094477
12.097923	694.360550	12.099495
12.396310	693.385720	12.104512
12.307160	688.394604	12.109530
12.378630	688.492719	12.114547
12.314810	691.627618	12.119565
12.308694	685.373224	12.124583
12.496314	704.427718	12.129600
12.584799	707.096876	12.134618
12.271178	714.125276	12.139635
12.714588	708.745197	12.144653
12.720178	722.340423	12.149671
12.794111	720.619341	12.154688
12.704935	702.925047	12.159706
12.310815	698.138750	12.164723
12.369903	701.071420	12.169741
12.381234	720.621633	12.174759
12.743726	715.847042	12.179776
12.867952	720.424343	12.184794
12.911177	720.953881	12.189811
13.150349	712.229082	12.194829
12.653399	705.572128	12.199847
12.756254	694.112204	12.204864
12.329505	688.753395	12.209882
12.675394	687.475442	12.214899
13.042616	696.239797	12.219917
12.825664	697.909595	12.224935
12.834782	692.462075	12.229952
12.417957	695.958167	12.234970
12.416824	692.664575	12.239987
12.835112	713.562266	12.245005
12.893521	722.621065	12.250023
12.871781	718.059696	12.255040
12.860811	725.849747	12.260058
12.799363	729.212594	12.265075
12.769421	721.152001	12.270093
12.607207	733.533760	12.275111
13.154488	732.907060	12.280128
13.087468	725.600592	12.285146
12.975288	725.242926	12.290163
13.083910	708.230004	12.295181
12.698092	709.020340	12.300199
13.033772	716.522683	12.305216
12.923257	730.204461	12.310234
12.572381	731.247658	12.315251
13.221164	722.718396	12.320269
13.078859	729.779847	12.325287
13.182654	723.904064	12.330304
13.349443	719.416982	12.335322
12.763145	713.712165	12.340339
12.942160	703.760791	12.345357
12.680871	716.227442	12.350375
12.881200	717.938373	12.355392
13.427101	724.818937	12.360410
12.888057	730.655217	12.365427
13.292718	717.415087	12.370445
13.018286	731.955850	12.375463
12.910975	731.865472	12.380480
13.253612	718.952521	12.385498
13.131232	732.137477	12.390515
13.314401	724.491566	12.395533
13.121089	723.787120	12.400551
12.705992	724.663009	12.405568
13.103998	724.691700	12.410586
13.051084	723.087679	12.415603
12.992534	711.867449	12.420621
13.035005	724.051536	12.425639
12.928588	725.790823	12.430656
12.808039	723.459463	12.435674
12.621237	723.086990	12.440691
13.224362	739.142189	12.445709
13.103521	755.410195	12.450727
12.967924	754.536751	12.455744
13.385440	750.487641	12.460762
13.070318	758.833162	12.465779
13.648647	751.303290	12.470797
13.254150	763.647556	12.475815
13.307206	762.660593	12.480832
13.539453	755.192751	12.485850
13.481810	755.337442	12.490867
13.454383	753.023332	12.495885
13.279759	754.901863	12.500903
12.940416	748.343194	12.505920
12.971780	744.866268	12.510938
12.880996	762.098932	12.515955
13.319894	750.815985	12.520973
13.517597	753.002525	12.525991
13.225259	752.628630	12.531008
13.361218	757.265413	12.536026
13.138440	775.406907	12.541043
13.653137	777.965345	12.546061
13.915633	790.920486	12.551079
13.603965	779.377967	12.556096
13.479536	760.628875	12.561114
13.402396	773.752046	12.566131
13.619016	785.818767	12.571149
13.685942	784.522436	12.576167
13.502211	788.731090	12.581184
13.909015	777.024329	12.586202
13.384961	773.524020	12.591219
13.759774	778.435806	12.596237
13.460798	783.339489	12.601255
13.692833	789.569732	12.606272
14.091797	781.460524	12.611290
13.587172	778.464449	12.616307
13.873725	755.606195	12.621325
13.519300	762.022510	12.626343
13.636267	769.635895	12.631360
13.940697	770.974890	12.636378
13.976945	768.379383	12.641395
13.694509	758.096536	12.646413
13.544743	755.121228	12.651431
13.550831	763.821019	12.656448
14.246992	774.931208	12.661466
13.614382	783.969044	12.666483
13.781643	776.217875	12.671501
13.988551	781.659800	12.676519
13.970901	783.324555	12.681536
14.051464	777.610070	12.686554
13.773123	763.353142	12.691571
13.759403	752.691568	12.696589
13.529704	766.984419	12.701607
13.709170	788.203631	12.706624
13.734734	782.046308	12.711642
13.670455	788.742917	12.716659
13.746380	779.225866	12.721677
13.708981	775.137126	12.726695
13.754201	778.059510	12.731712
13.843088	784.261489	12.736730
13.975000	780.378162	12.741747
13.769507	782.522029	12.746765
13.765478	781.067773	12.751783
13.942837	800.701612	12.756800
14.355646	806.973577	12.761818
14.174995	810.975046	12.766835
14.037306	799.573773	12.771853
13.967788	795.095879	12.776871
14.078151	809.529691	12.781888
14.215600	804.903355	12.786906
14.009926	818.149418	12.791923
14.508555	806.197913	12.796941
14.310193	798.171468	12.801959
14.312934	784.868314	12.806976
14.257202	780.525142	12.811994
13.795542	783.144475	12.817011
13.759967	792.536576	12.822029
14.407049	796.147447	12.827047
14.153220	802.404215	12.832064
14.026058	805.313813	12.837082
14.468769	819.794170	12.842099
14.290458	812.286811	12.847117
14.008649	808.379471	12.852135
14.092392	812.180867	12.857152
14.354219	806.083226	12.862170
14.107788	813.872549	12.867187
14.250490	808.931186	12.872205
14.197291	804.573022	12.877223
14.176669	811.059666	12.882240
14.628599	801.379163	12.887258
14.496268	808.614974	12.892275
14.570596	805.021870	12.897293
14.757421	806.492541	12.902311
14.230067	803.528570	12.907328
14.715053	803.966851	12.912346
14.439698	807.479696	12.917363
14.514014	810.595289	12.922381
14.635261	806.946387	12.927399
14.365592	812.357009	12.932416
14.540098	807.008039	12.937434
14.601248	808.092850	12.942451
14.242936	809.884488	12.947469
14.328387	811.099520	12.952487
14.017781	821.200138	12.957504
14.482691	803.637195	12.962522
14.484163	811.049658	12.967539
14.099998	819.523568	12.972557
14.680782	824.205210	12.977575
14.993315	841.619589	12.982592
15.080821	825.386767	12.987610
14.442642	817.373695	12.992627
14.541345	809.339783	12.997645
14.870925	802.517969	13.002663
14.451244	813.199606	13.007680
14.747147	815.994664	13.012698
14.597909	832.921356	13.017715
14.907309	839.474223	13.022733
15.228285	832.948688	13.027751
14.838599	816.657499	13.032768
15.090926	812.532190	13.037786
14.742850	807.414629	13.042803
14.713529	809.880096	13.047821
14.630579	801.862094	13.052839
14.408739	815.075400	13.057856
14.605943	827.894935	13.062874
14.780512	834.237856	13.067891
14.716696	836.091355	13.072909
14.909254	831.423604	13.077927
15.189616	840.565398	13.082944
15.146810	835.750015	13.087962
14.893039	839.368344	13.092979
14.931340	848.315985	13.097997
15.301088	833.829633	13.103015
15.247913	845.999734	13.108032
15.303170	832.759493	13.113050
14.937578	814.681338	13.118067
14.934810	812.591471	13.123085
15.010664	800.952485	13.128103
14.812049	807.962276	13.133120
15.457925	819.777244	13.138138
15.202303	817.917818	13.143155
14.969860	818.208378	13.148173
14.980674	808.917827	13.153191
14.819502	821.629386	13.158208
15.020051	822.692296	13.163226
15.049899	834.571884	13.168243
15.104440	839.298154	13.173261
15.410183	831.326398	13.178279
15.420073	835.858102	13.183296
15.078761	836.417858	13.188314
15.495304	845.636705	13.193331
15.111247	834.831292	13.198349
15.570921	822.339404	13.203367
15.126839	832.721567	13.208384
15.382143	823.768062	13.213402
15.240522	824.694335	13.218419
15.287956	825.536943	13.223437
15.231740	833.712868	13.228455
15.266847	843.038968	13.233472
15.315199	835.165734	13.238490
15.304660	843.893126	13.243507
15.184374	852.309973	13.248525
15.520081	837.482028	13.253543
15.596015	844.197566	13.258560
15.298263	836.092682	13.263578
15.310845	835.271464	13.268595
15.166415	835.675395	13.273613
15.462490	831.203091	13.278631
15.209647	840.423730	13.283648
15.239656	837.088338	13.288666
15.232692	841.991714	13.293683
15.399251	834.352043	13.298701
15.412614	838.400521	13.303719
15.427059	843.994411	13.308736
15.351006	834.446590	13.313754
15.478910	843.965581	13.318771
15.410627	858.001878	13.323789
15.215047	866.782363	13.328807
15.648143	868.440989	13.333824
15.706080	871.208536	13.338842
15.926860	864.873980	13.343859
15.912103	873.621378	13.348877
16.390268	863.696740	13.353895
15.787697	850.779576	13.358912
15.759414	839.885326	13.363930
15.993227	843.109547	13.368947
15.754334	837.244012	13.373965
15.479515	836.120797	13.378983
15.681792	838.706964	13.384000
15.695471	830.491067	13.389018
16.211701	829.463622	13.394035
15.716314	828.707228	13.399053
15.601887	828.246000	13.404071
15.803718	832.463652	13.409088
15.666978	834.913447	13.414106
15.759629	840.509346	13.419123
15.646586	856.426184	13.424141
16.147338	851.775500	13.429159
16.058451	866.132522	13.434176
16.028469	858.131704	13.439194
16.057781	850.436409	13.444211
15.949727	852.105907	13.449229
16.112670	847.397388	13.454247
15.905879	835.895726	13.459264
15.685550	845.542064	13.464282
16.085314	854.702281	13.469299
16.222091	856.512330	13.474317
16.036178	857.971110	13.479335
16.151595	856.149447	13.484352
16.284165	858.598744	13.489370
16.265451	844.356226	13.494387
15.830363	843.655591	13.499405
16.204037	837.877194	13.504423
16.490745	839.318731	13.509440
16.217123	829.053274	13.514458
16.221981	829.741917	13.519475
16.000460	820.807925	13.524493
15.864693	828.472244	13.529511
16.149966	840.368592	13.534528
16.193854	853.592257	13.539546
16.160088	850.368993	13.544563
16.091297	853.070124	13.549581
16.228863	846.356855	13.554599
16.384127	857.744064	13.559616
16.102990	855.361720	13.564634
16.349248	858.523257	13.569651
16.229983	866.348239	13.574669
16.543314	858.666931	13.579687
16.352760	865.565576	13.584704
16.595403	869.108403	13.589722
16.520416	864.314874	13.594739
16.618132	861.281243	13.599757
16.413846	857.449631	13.604775
16.687532	858.553186	13.609792
16.393524	853.691997	13.614810
16.393091	860.487115	13.619827
16.502133	863.546970	13.624845
16.446656	859.135627	13.629863
16.540942	867.350817	13.634880
16.809493	863.494054	13.639898
16.844670	864.433571	13.644915
16.369116	866.750903	13.649933
16.710901	861.509641	13.654951
16.588585	861.851646	13.659968
16.426661	868.055823	13.664986
16.559294	860.535925	13.670003
16.647197	868.230152	13.675021
16.784484	857.799787	13.680039
16.844578	858.574162	13.685056
16.407385	864.882578	13.690074
16.249248	853.244112	13.695091
16.253847	862.607558	13.700109
16.616590	859.695386	13.705127
16.837232	856.756749	13.710144
16.489314	866.365175	13.715162
16.718237	852.153293	13.720179
16.460276	861.161811	13.725197
16.683780	858.981716	13.730215
17.026044	871.809942	13.735232
16.781693	876.760905	13.740250
16.871533	867.504475	13.745267
16.820105	881.803737	13.750285
17.132298	878.078713	13.755303
16.999685	866.628127	13.760320
16.961003	871.809191	13.765338
17.091637	858.398974	13.770355
16.860710	864.671265	13.775373
16.934927	853.921836	13.780391
16.921511	864.141372	13.785408
16.920420	879.259027	13.790426
17.202333	886.693589	13.795443
16.822298	891.448531	13.800461
16.989416	889.334065	13.805479
17.655775	886.373188	13.810496
17.304053	881.356200	13.815514
17.336540	852.606701	13.820531
16.651310	853.437175	13.825549
16.900673	858.902411	13.830567
17.305466	862.678609	13.835584
16.873507	884.627120	13.840602
17.260613	873.154245	13.845619
17.105130	889.665124	13.850637
17.237055	882.263437	13.855655
17.484717	890.626462	13.860672
17.227338	881.868443	13.865690
17.430784	875.041895	13.870707
17.512872	887.088061	13.875725
17.084631	870.274879	13.880743
17.445415	873.519417	13.885760
17.197808	877.031227	13.890778
17.174662	873.325908	13.895795
17.041636	882.567674	13.900813
17.009551	881.575906	13.905831
17.209618	878.595004	13.910848
17.287292	884.267410	13.915866
17.403539	879.596928	13.920883
17.293398	884.745344	13.925901
17.268362	885.176354	13.930919
17.082587	874.321545	13.935936
16.947752	885.030469	13.940954
17.713256	889.526039	13.945971
17.638387	898.887706	13.950989
17.620190	898.195985	13.956007
17.872143	898.464993	13.961024
17.642279	892.930997	13.966042
17.628724	882.657477	13.971059
17.558121	881.095737	13.976077
17.521897	884.143432	13.981095
17.617329	870.237483	13.986112
17.328081	888.423972	13.991130
17.976094	894.785760	13.996147
17.908568	902.259297	14.001165
17.815146	893.860323	14.006183
17.715230	873.004380	14.011200
17.473567	882.162566	14.016218
18.226882	892.069734	14.021235
17.843776	873.762531	14.026253
17.548067	877.846452	14.031271
17.800239	873.006620	14.036288
17.924679	892.235580	14.041306
17.827636	881.997931	14.046323
17.900372	891.649704	14.051341
18.056847	896.425250	14.056359
18.205093	887.549275	14.061376
17.438067	883.616756	14.066394
18.028691	890.288424	14.071411
17.870374	911.729873	14.076429
18.069723	907.607800	14.081447
18.304164	905.744376	14.086464
17.580803	898.403997	14.091482
18.035973	897.525628	14.096499
17.739094	910.708136	14.101517
17.695952	907.993475	14.106535
18.398496	905.317533	14.111552
18.289878	907.838271	14.116570
18.130419	896.288176	14.121587
18.207674	898.138794	14.126605
18.171794	901.620667	14.131623
18.130791	901.398447	14.136640
17.989957	903.359191	14.141658
17.866972	900.573111	14.146675
18.051145	905.110227	14.151693
18.088042	902.169331	14.156711
18.341150	891.771731	14.161728
18.097482	898.551633	14.166746
18.270732	896.068058	14.171763
18.153699	904.013157	14.176781
18.068359	897.702901	14.181799
18.478982	891.055809	14.186816
18.209426	906.160467	14.191834
18.320254	891.544503	14.196851
18.338970	895.127565	14.201869
18.386616	902.339522	14.206887
18.571749	894.275901	14.211904
18.236186	902.998094	14.216922
18.194845	885.449207	14.221939
18.426799	896.272984	14.226957
18.049196	894.153447	14.231975
18.358812	908.989376	14.236992
18.400849	932.027521	14.242010
18.431976	926.043228	14.247027
18.790874	922.274635	14.252045
18.423434	932.787474	14.257063
18.501195	925.905735	14.262080
18.507285	927.914590	14.267098
18.622511	924.154064	14.272115
18.851980	923.771708	14.277133
18.661166	928.829959	14.282151
19.070578	923.701882	14.287168
18.840019	928.774194	14.292186
18.978388	926.901087	14.297203
18.786834	909.827024	14.302221
18.757903	917.114658	14.307239
18.963184	893.814167	14.312256
18.559656	897.526201	14.317274
18.523583	899.709743	14.322291
18.834972	915.045755	14.327309
18.991008	913.161063	14.332327
19.165012	914.314985	14.337344
18.964174	903.343364	14.342362
18.717083	901.928557	14.347379
19.095878	910.061621	14.352397
18.943917	905.944574	14.357415
18.374348	907.673964	14.362432
18.845777	917.202650	14.367450
18.776532	917.087464	14.372467
18.924409	923.424213	14.377485
18.730928	920.736806	14.382503
19.477807	917.786604	14.387520
19.498948	921.200381	14.392538
19.194355	922.494576	14.397555
19.248754	918.201235	14.402573
19.156709	925.872535	14.407591
19.191378	912.929321	14.412608
18.988252	917.210903	14.417626
19.157388	916.502727	14.422643
19.285285	914.887642	14.427661
19.139248	921.223849	14.432679
19.535044	912.837552	14.437696
19.152972	915.892918	14.442714
19.396828	928.433959	14.447731
19.776763	917.640554	14.452749
19.134022	901.860840	14.457767
18.981961	893.753847	14.462784
18.949614	909.084570	14.467802
19.323517	911.570681	14.472819
19.393734	907.838477	14.477837
18.946882	921.127320	14.482855
19.386599	907.354082	14.487872
19.508841	921.632497	14.492890
19.370389	920.938247	14.497907
19.304970	913.112946	14.502925
19.196536	916.947372	14.507943
19.456649	915.686754	14.512960
19.335706	914.264836	14.517978
19.055227	910.240326	14.522995
19.706135	920.508549	14.528013
19.191598	917.215675	14.533031
19.277414	920.747083	14.538048
19.335436	928.484081	14.543066
19.266073	947.021218	14.548083
19.736780	950.320796	14.553101
19.484452	941.869373	14.558119
19.849802	949.670054	14.563136
19.665782	946.662980	14.568154
19.814659	948.618668	14.573171
20.024438	953.861762	14.578189
19.595044	956.944263	14.583207
20.134288	939.860568	14.588224
20.112009	940.892277	14.593242
19.718603	938.819836	14.598259
19.818727	932.142257	14.603277
19.537374	938.041449	14.608295
19.973503	939.261412	14.613312
19.827622	946.318042	14.618330
19.993619	939.854738	14.623347
20.152005	937.277560	14.628365
19.882817	937.487595	14.633383
20.034646	934.970949	14.638400
20.147106	942.092668	14.643418
19.971301	939.061008	14.648435
20.355471	934.275675	14.653453
19.796520	922.778720	14.658471
20.044058	927.830522	14.663488
19.880517	927.559305	14.668506
19.933829	942.434559	14.673523
20.201857	936.190571	14.678541
19.827775	941.792536	14.683559
20.148512	937.872391	14.688576
20.330442	936.893210	14.693594
20.128315	941.251007	14.698611
20.305644	941.509146	14.703629
20.321541	947.133934	14.708647
20.242064	936.399661	14.713664
20.343664	942.455905	14.718682
20.022723	946.856605	14.723699
20.308253	926.519809	14.728717
20.063918	944.499330	14.733735
20.175126	940.139492	14.738752
20.349826	941.514945	14.743770
20.169438	944.470388	14.748787
20.327187	940.310708	14.753805
20.213906	947.984748	14.758823
20.230650	941.813075	14.763840
20.037927	947.214152	14.768858
19.973805	948.890163	14.773875
20.488448	967.171178	14.778893
20.346650	973.455524	14.783911
20.663035	978.361303	14.788928
20.826537	970.264218	14.793946
20.833392	977.802242	14.798963
21.063415	968.621354	14.803981
20.353707	953.001095	14.808999
20.603710	969.292166	14.814016
20.916637	966.376414	14.819034
20.300467	959.068253	14.824051
20.519946	962.357862	14.829069
20.881004	971.886748	14.834087
20.981338	971.898593	14.839104
20.945308	967.007247	14.844122
20.420011	961.854809	14.849139
20.760124	962.981623	14.854157
20.838479	982.278953	14.859175
20.887380	975.485433	14.864192
20.972746	979.064171	14.869210
20.814694	978.438909	14.874227
21.214565	971.209731	14.879245
20.791398	950.835931	14.884263
20.343733	946.875708	14.889280
20.662651	954.950997	14.894298
20.224738	968.389181	14.899315
20.624976	966.017214	14.904333
20.692610	969.704787	14.909351
20.494956	965.372465	14.914368
21.340199	971.079607	14.919386
21.056769	986.494501	14.924403
21.407531	973.399293	14.929421
21.139524	978.504986	14.934439
20.864930	974.480272	14.939456
21.085344	966.161175	14.944474
20.865842	983.464217	14.949491
21.269874	987.451193	14.954509
21.230594	995.447634	14.959527
21.597413	993.701250	14.964544
21.484533	989.298981	14.969562
21.047554	984.754719	14.974579
21.374224	983.315760	14.979597
21.324960	987.645896	14.984615
20.930996	973.036280	14.989632
21.510601	978.901973	14.994650
21.275159	988.502086	14.999667
21.622283	993.024449	15.004685
21.629664	998.172732	15.009703
21.790369	992.404349	15.014720
21.363076	975.412948	15.019738
21.102628	973.844448	15.024755
21.771870	969.405189	15.029773
21.485623	976.026041	15.034791
21.312558	976.486290	15.039808
21.902160	983.771529	15.044826
21.608792	980.793972	15.049843
21.891623	968.053310	15.054861
21.323049	964.438679	15.059879
21.280647	968.247618	15.064896
21.681331	978.581722	15.069914
21.579395	985.947616	15.074931
21.750437	989.362963	15.079949
21.992617	988.203730	15.084967
21.742650	987.954697	15.089984
21.951552	981.789376	15.095002
21.591612	983.795072	15.100019
21.807299	988.054171	15.105037
21.975971	984.868614	15.110055
21.939829	977.916347	15.115072
21.714402	985.401898	15.120090
21.735361	986.860684	15.125107
21.907173	992.932485	15.130125
21.998070	990.997155	15.135143
21.987376	983.076146	15.140160
21.977698	982.536153	15.145178
21.970386	982.552438	15.150195
22.090843	982.974712	15.155213
21.827698	979.438238	15.160231
21.788668	987.374399	15.165248
22.179755	987.086928	15.170266
21.724948	992.669602	15.175283
21.758043	985.933810	15.180301
21.919929	990.161663	15.185319
21.569234	988.673456	15.190336
21.338918	985.728369	15.195354
21.443541	1008.866890	15.200371
21.881697	1007.660244	15.205389
21.679566	1010.110659	15.210407
22.149604	1015.708694	15.215424
22.219839	1008.127800	15.220442
22.279504	1021.340335	15.225459
22.234488	1025.604820	15.230477
22.929380	1022.127403	15.235495
22.722424	1021.692513	15.240512
22.674948	1007.703417	15.245530
22.535923	1011.058699	15.250547
22.787710	1008.724300	15.255565
22.617133	1006.367324	15.260583
22.679363	1006.455948	15.265600
22.681480	997.919842	15.270618
22.904218	1003.603310	15.275635
22.765783	1001.603595	15.280653
22.738938	1006.367408	15.285671
22.389708	1002.337329	15.290688
22.890237	988.179557	15.295706
22.545265	983.749188	15.300723
22.829546	982.194812	15.305741
22.546669	980.521368	15.310759
22.447378	986.108553	15.315776
22.639322	987.479974	15.320794
22.649975	993.723731	15.325811
23.072957	994.806905	15.330829
22.788088	1003.159752	15.335847
22.757000	1000.973371	15.340864
22.765475	1005.101439	15.345882
22.563481	997.467601	15.350899
22.798735	1004.574921	15.355917
22.804236	1001.104188	15.360935
22.778976	1002.830068	15.365952
23.180776	990.136614	15.370970
23.007562	996.871035	15.375987
23.012761	997.363575	15.381005
22.722025	1002.500204	15.386023
22.616957	999.956798	15.391040
22.648797	997.035225	15.396058
22.428720	1005.331676	15.401075
22.747399	1008.039931	15.406093
22.895877	1015.701761	15.411111
22.918297	1028.964168	15.416128
23.537288	1028.043706	15.421146
23.395496	1033.040726	15.426163
23.436465	1025.206018	15.431181
23.557919	1021.890089	15.436199
23.196895	1018.844990	15.441216
23.396031	994.667054	15.446234
23.144970	1000.532515	15.451251
23.390904	1002.607566	15.456269
23.530025	1009.793796	15.461287
23.034486	1004.456502	15.466304
23.389467	1007.274096	15.471322
23.405355	1024.380338	15.476339
23.532108	1020.998967	15.481357
23.332498	1020.901037	15.486375
23.328218	1024.286764	15.491392
23.196651	1023.029974	15.496410
23.063165	1020.539300	15.501427
23.440378	1032.039485	15.506445
23.424195	1013.321372	15.511463
23.439758	1018.179343	15.516480
23.432227	1017.889770	15.521498
23.569435	1023.514182	15.526515
23.733522	1018.675507	15.531533
23.745576	1010.055075	15.536551
23.314769	1023.545671	15.541568
23.928002	1022.752142	15.546586
23.702875	1032.325771	15.551603
23.635603	1025.714057	15.556621
23.651535	1025.233599	15.561639
23.235504	1019.204028	15.566656
23.561798	1039.684340	15.571674
24.023300	1037.197892	15.576691
23.789424	1051.746411	15.581709
24.029159	1047.606197	15.586727
23.899592	1050.327269	15.591744
24.091647	1047.710640	15.596762
24.071906	1056.045596	15.601779
23.989483	1051.046162	15.606797
24.129977	1052.010769	15.611815
23.874888	1048.369011	15.616832
23.987951	1051.395957	15.621850
24.053594	1056.826333	15.626867
23.957769	1049.833919	15.631885
24.293929	1050.271657	15.636903
24.074358	1057.161413	15.641920
24.301329	1049.425022	15.646938
24.190811	1051.633904	15.651955
24.068109	1052.235023	15.656973
24.446937	1049.822890	15.661991
24.539711	1053.010276	15.667008
24.353302	1042.784563	15.672026
24.067691	1054.806710	15.677043
24.035640	1049.299742	15.682061
24.280317	1045.955136	15.687079
24.136194	1048.430990	15.692096
24.111009	1050.361185	15.697114
24.112165	1060.801264	15.702131
23.954797	1051.808485	15.707149
24.324578	1048.450249	15.712167
24.116760	1057.919457	15.717184
24.445975	1070.154363	15.722202
24.690649	1074.141767	15.727219
24.738765	1074.591770	15.732237
24.989012	1070.454927	15.737255
24.865795	1056.543680	15.742272
24.691806	1046.293861	15.747290
24.667333	1048.738091	15.752307
24.804483	1045.532546	15.757325
24.690239	1038.095960	15.762343
24.400808	1048.896341	15.767360
24.573535	1039.887491	15.772378
25.108268	1051.960797	15.777395
24.645957	1054.565715	15.782413
24.864956	1050.945449	15.787431
24.643654	1062.687672	15.792448
25.279139	1059.084657	15.797466
25.090288	1043.000514	15.802483
24.727128	1045.734282	15.807501
25.304459	1037.863506	15.812519
24.876368	1049.145099	15.817536
25.134967	1039.679919	15.822554
24.823053	1033.575229	15.827571
24.912118	1042.382693	15.832589
24.873312	1047.111098	15.837607
24.898342	1058.649937	15.842624
25.308857	1060.154850	15.847642
25.647654	1062.653492	15.852659
25.256404	1052.516808	15.857677
25.375578	1037.048175	15.862695
25.273471	1050.085168	15.867712
25.072382	1035.659295	15.872730
25.130511	1038.459516	15.877747
25.077994	1037.523481	15.882765
25.375249	1045.304779	15.887783
25.379789	1059.536278	15.892800
25.154702	1062.677091	15.897818
25.231072	1054.403452	15.902835
25.373284	1069.014510	15.907853
25.311965	1058.159040	15.912871
25.177196	1074.174972	15.917888
25.419835	1067.229650	15.922906
25.420572	1070.023239	15.927923
25.393449	1069.791633	15.932941
25.573717	1052.225544	15.937959
25.654430	1064.768514	15.942976
25.444175	1067.416733	15.947994
25.549065	1068.174646	15.953011
25.193861	1072.231856	15.958029
25.592406	1066.071318	15.963047
25.232323	1064.778746	15.968064
25.202006	1058.874651	15.973082
25.454682	1088.329090	15.978099
25.660343	1091.858802	15.983117
25.978239	1094.171940	15.988135
25.818356	1102.365960	15.993152
25.945307	1088.493964	15.998170
25.956521	1093.249927	16.003187
25.888125	1097.577750	16.008205
26.255881	1082.322232	16.013223
25.936522	1081.761864	16.018240
25.941696	1089.616745	16.023258
26.057825	1087.681556	16.028275
25.981575	1086.706536	16.033293
26.217982	1084.110115	16.038311
25.954895	1091.625574	16.043328
26.106145	1090.630992	16.048346
26.213572	1084.678489	16.053363
26.281364	1093.864295	16.058381
26.333806	1092.219562	16.063399
26.133983	1089.254052	16.068416
26.105690	1092.070562	16.073434
26.491632	1081.435099	16.078451
26.682409	1085.538513	16.083469
26.535571	1075.878646	16.088487
26.580195	1053.905257	16.093504
25.932881	1059.032054	16.098522
26.233864	1063.397125	16.103539
26.320411	1077.932372	16.108557
26.420478	1076.760840	16.113575
26.572040	1088.992109	16.118592
26.484120	1083.399502	16.123610
26.678238	1080.847484	16.128627
26.211916	1077.418249	16.133645
26.844447	1082.122111	16.138663
26.552889	1079.575322	16.143680
26.685036	1077.900858	16.148698
26.522947	1081.472565	16.153715
26.532534	1088.694455	16.158733
26.498692	1086.220733	16.163751
26.800964	1081.307977	16.168768
26.255019	1086.386502	16.173786
26.606762	1086.474430	16.178803
26.500413	1093.832838	16.183821
26.296546	1083.295433	16.188839
26.439775	1083.624967	16.193856
26.658055	1099.891508	16.198874
26.647757	1101.564135	16.203891
26.757722	1106.102575	16.208909
26.575100	1112.115795	16.213927
26.827370	1115.428746	16.218944
27.004211	1119.304564	16.223962
26.925659	1110.666010	16.228979
26.731369	1120.341276	16.233997
26.703287	1113.917911	16.239015
26.945517	1111.099662	16.244032
27.014100	1112.078150	16.249050
27.326272	1104.591394	16.254067
27.185521	1118.199784	16.259085
27.189641	1108.221208	16.264103
27.311563	1105.791768	16.269120
26.994626	1102.514950	16.274138
27.205755	1111.141616	16.279155
27.206962	1121.185679	16.284173
27.427161	1132.954845	16.289191
27.366218	1131.722177	16.294208
27.441704	1121.605009	16.299226
27.667774	1116.833595	16.304243
27.199107	1108.033271	16.309261
27.429432	1122.299485	16.314279
27.972204	1132.081837	16.319296
27.721836	1127.010978	16.324314
27.721349	1117.322914	16.329331
27.507485	1111.736191	16.334349
27.403999	1104.561168	16.339367
27.276477	1104.180050	16.344384
27.014182	1118.138869	16.349402
27.715341	1124.945483	16.354419
27.525702	1135.216425	16.359437
27.864210	1141.983100	16.364455
27.997487	1136.366444	16.369472
28.095186	1140.058921	16.374490
28.230536	1135.124578	16.379507
27.891350	1131.151461	16.384525
27.759274	1126.518087	16.389543
27.829698	1129.485574	16.394560
27.668288	1139.035333	16.399578
28.081818	1123.558423	16.404595
27.523494	1146.751810	16.409613
27.997931	1132.966325	16.414631
28.024703	1136.130800	16.419648
27.781303	1138.979394	16.424666
27.570665	1135.832995	16.429683
27.453949	1136.279587	16.434701
27.964937	1134.648287	16.439719
27.866401	1148.324120	16.444736
28.046804	1165.600121	16.449754
28.315230	1171.197347	16.454771
28.257699	1174.669875	16.459789
28.167296	1174.748736	16.464807
28.122075	1164.349174	16.469824
28.136080	1166.471313	16.474842
28.430324	1160.982714	16.479859
28.209110	1162.391463	16.484877
28.115799	1163.053464	16.489895
28.548517	1164.060239	16.494912
27.911681	1160.944644	16.499930
28.344748	1159.828198	16.504947
28.084867	1166.303430	16.509965
28.338711	1182.526769	16.514983
28.616936	1180.922985	16.520000
28.649886	1194.160956	16.525018
28.638696	1187.628073	16.530035
28.771547	1188.710487	16.535053
28.785519	1185.148943	16.540071
28.693022	1191.267738	16.545088
28.352790	1186.327092	16.550106
29.004834	1177.407292	16.555123
29.131718	1189.442732	16.560141
28.726388	1183.107789	16.565159
28.985207	1180.963533	16.570176
28.931005	1169.516273	16.575194
28.985287	1151.707163	16.580211
28.805183	1155.811381	16.585229
28.714748	1161.355038	16.590247
29.231544	1166.857201	16.595264
28.965471	1171.244941	16.600282
28.976302	1178.493437	16.605299
29.214653	1181.877210	16.610317
29.276274	1183.530063	16.615335
28.979860	1160.937030	16.620352
28.879430	1173.341585	16.625370
29.323845	1187.529103	16.630387
29.022189	1184.666261	16.635405
28.478150	1183.660823	16.640423
29.434829	1182.733649	16.645440
29.327402	1186.306564	16.650458
29.455287	1174.844897	16.655475
29.095475	1177.908832	16.660493
29.422891	1182.052243	16.665511
29.521002	1179.068876	16.670528
29.114927	1187.876918	16.675546
29.187337	1181.465230	16.680563
29.351569	1186.291549	16.685581
29.201924	1189.163209	16.690599
29.248702	1185.271439	16.695616
29.282098	1208.983061	16.700634
29.684885	1207.877531	16.705651
29.893321	1213.900837	16.710669
29.662148	1207.776802	16.715687
29.619227	1208.545419	16.720704
29.341643	1214.125990	16.725722
29.749263	1215.254637	16.730739
29.698768	1214.756040	16.735757
29.708203	1213.607379	16.740775
30.019393	1203.155860	16.745792
29.733995	1215.158411	16.750810
29.516532	1215.340987	16.755827
29.750485	1207.867133	16.760845
29.525822	1215.453452	16.765863
30.022415	1212.706450	16.770880
29.860710	1214.097869	16.775898
29.662864	1207.812021	16.780915
29.960678	1228.456745	16.785933
30.153814	1238.867123	16.790951
30.496994	1234.420762	16.795968
30.274752	1238.655992	16.800986
30.355321	1229.758352	16.806003
30.395599	1218.831617	16.811021
30.281813	1209.102022	16.816039
30.479919	1203.700978	16.821056
30.330004	1202.201550	16.826074
30.358279	1198.310872	16.831091
30.579600	1202.333671	16.836109
30.285832	1200.895070	16.841127
30.659438	1200.682536	16.846144
30.029552	1205.820273	16.851162
30.516964	1198.826094	16.856179
30.433428	1202.197819	16.861197
30.253832	1214.768661	16.866215
30.503837	1227.257353	16.871232
30.446947	1238.996106	16.876250
30.258619	1232.303564	16.881267
30.826331	1232.345496	16.886285
30.806908	1241.154108	16.891303
30.741959	1230.061724	16.896320
30.770327	1236.225088	16.901338
30.747413	1231.208262	16.906355
31.348417	1230.824613	16.911373
31.000305	1232.081945	16.916391
30.896544	1230.737071	16.921408
30.812948	1227.827483	16.926426
30.756246	1231.316421	16.931443
30.931012	1235.157179	16.936461
30.809312	1232.001938	16.941479
30.790690	1228.765457	16.946496
30.993539	1238.477002	16.951514
31.040289	1229.212531	16.956531
31.061555	1232.438565	16.961549
30.676314	1231.974531	16.966567
30.611130	1227.290288	16.971584
30.957191	1229.948774	16.976602
30.990900	1231.843256	16.981619
31.078324	1231.992669	16.986637
30.773638	1254.421401	16.991655
30.870846	1253.763702	16.996672
30.875047	1264.368765	17.001690
31.198288	1258.277707	17.006707
31.015618	1254.799494	17.011725
30.887932	1263.581165	17.016743
31.426597	1270.682461	17.021760
31.543714	1288.280488	17.026778
31.594984	1291.601564	17.031795
31.797887	1281.162806	17.036813
31.096922	1286.950514	17.041831
31.672255	1276.086318	17.046848
31.978153	1280.666380	17.051866
31.760995	1276.877345	17.056883
32.047438	1271.750226	17.061901
32.031503	1278.141017	17.066919
32.297382	1261.165621	17.071936
31.930389	1254.392027	17.076954
31.917631	1249.598310	17.081971
31.843228	1243.271535	17.086989
31.669353	1240.802080	17.092007
31.806654	1242.153832	17.097024
31.809943	1244.265158	17.102042
31.900892	1248.631991	17.107059
32.317057	1260.077867	17.112077
32.038860	1267.536858	17.117095
32.073036	1252.476171	17.122112
31.935346	1251.567218	17.127130
32.238482	1273.711871	17.132147
32.263343	1273.083474	17.137165
32.212978	1282.581863	17.142183
32.501922	1273.028448	17.147200
32.173469	1267.114982	17.152218
32.304709	1269.368507	17.157235
32.265518	1269.899900	17.162253
32.430247	1274.614357	17.167271
32.582356	1267.230798	17.172288
32.435392	1270.813823	17.177306
32.435340	1268.112435	17.182323
32.585618	1262.227965	17.187341
32.420956	1271.283079	17.192359
32.673533	1275.101121	17.197376
32.202585	1271.646624	17.202394
32.674676	1276.726318	17.207411
32.935482	1273.492376	17.212429
32.585024	1270.335243	17.217447
32.228614	1269.507387	17.222464
32.748815	1268.911139	17.227482
32.704019	1265.828981	17.232499
33.070256	1269.144748	17.237517
32.779700	1267.930406	17.242535
32.902414	1272.908506	17.247552
33.006279	1270.448959	17.252570
32.728619	1272.949716	17.257587
32.728644	1272.998250	17.262605
32.819107	1282.561506	17.267623
33.027437	1273.778509	17.272640
32.519783	1273.374900	17.277658
32.489627	1280.286538	17.282675
33.073802	1278.968295	17.287693
32.874524	1297.782870	17.292711
32.664992	1301.551455	17.297728
32.845704	1309.765168	17.302746
33.083776	1307.845980	17.307763
33.084763	1303.569251	17.312781
32.785825	1306.453449	17.317799
32.780221	1306.110404	17.322816
33.105712	1316.367819	17.327834
33.193662	1326.872051	17.332851
33.234590	1330.571218	17.337869
33.433059	1331.632148	17.342887
33.310724	1334.534351	17.347904
33.818232	1335.972052	17.352922
33.574135	1336.041325	17.357939
33.657630	1329.721833	17.362957
33.339554	1331.018291	17.367975
33.648649	1327.572410	17.372992
33.802834	1328.832400	17.378010
33.641016	1321.470089	17.383027
33.513027	1318.920977	17.388045
33.597975	1324.734070	17.393063
33.565057	1319.265731	17.398080
33.857691	1324.513737	17.403098
33.913105	1345.768035	17.408115
33.937897	1349.387204	17.413133
33.914408	1350.975429	17.418151
33.986485	1349.212066	17.423168
34.160239	1343.122500	17.428186
34.123530	1344.033400	17.433203
34.685001	1341.763025	17.438221
34.234024	1332.890351	17.443239
34.026821	1321.658861	17.448256
34.319805	1321.918722	17.453274
34.292214	1326.218986	17.458291
34.658857	1318.091232	17.463309
34.459489	1319.200321	17.468327
34.503447	1309.707135	17.473344
34.685852	1308.350302	17.478362
34.509690	1321.446634	17.483379
34.589941	1304.749953	17.488397
34.563631	1314.435319	17.493415
34.693444	1309.297511	17.498432
34.725608	1315.763816	17.503450
34.913166	1318.705645	17.508467
34.842645	1305.857472	17.513485
34.741120	1308.129467	17.518503
34.525653	1312.284463	17.523520
34.619933	1301.092828	17.528538
34.727346	1308.869082	17.533555
35.007205	1294.929064	17.538573
34.675144	1314.225871	17.543591
34.848727	1304.891535	17.548608
35.142296	1304.585170	17.553626
34.918140	1308.843963	17.558643
34.852741	1302.572365	17.563661
34.938478	1303.687391	17.568679
34.750269	1316.240844	17.573696
34.872867	1320.122545	17.578714
34.544130	1315.588606	17.583731
34.594728	1309.096620	17.588749
34.997722	1311.838212	17.593767
34.879064	1323.820717	17.598784
34.791163	1334.759182	17.603802
34.731447	1339.308859	17.608819
34.855356	1325.595420	17.613837
35.085488	1327.744785	17.618855
35.018316	1326.708011	17.623872
35.171207	1330.248091	17.628890
35.035007	1357.341106	17.633907
35.469582	1367.348607	17.638925
35.697470	1358.882396	17.643943
35.253286	1356.916728	17.648960
35.634420	1355.189982	17.653978
35.593315	1347.788379	17.658995
35.776855	1345.032169	17.664013
35.652796	1361.693462	17.669031
35.867610	1359.657254	17.674048
35.730087	1350.205905	17.679066
35.807159	1348.522029	17.684083
35.761424	1352.277677	17.689101
35.641407	1351.345713	17.694119
35.396314	1353.875341	17.699136
35.753301	1349.233357	17.704154
35.556007	1353.250318	17.709171
35.718389	1359.931295	17.714189
35.606642	1356.982250	17.719207
35.912504	1362.902869	17.724224
36.207027	1375.170534	17.729242
35.970345	1387.893879	17.734259
36.033670	1381.871401	17.739277
36.335558	1379.476291	17.744295
36.023525	1383.396906	17.749312
36.475625	1373.225873	17.754330
36.407035	1382.619862	17.759347
36.442226	1381.633063	17.764365
36.441038	1376.509444	17.769383
36.092150	1377.971242	17.774400
36.194859	1382.044437	17.779418
36.049565	1385.959884	17.784435
36.403813	1373.681860	17.789453
36.338666	1380.089897	17.794471
36.132046	1381.031295	17.799488
36.217406	1374.755570	17.804506
36.260308	1397.445845	17.809523
36.122088	1393.829927	17.814541
36.553214	1400.782952	17.819559
36.817521	1410.411988	17.824576
36.735241	1401.044766	17.829594
36.728519	1408.447849	17.834611
36.762410	1401.784972	17.839629
36.818409	1407.500135	17.844647
36.877158	1410.323156	17.849664
37.280692	1386.767841	17.854682
36.973971	1393.469423	17.859699
37.084481	1400.696794	17.864717
37.135123	1402.740853	17.869735
36.988144	1398.058684	17.874752
36.985359	1399.814744	17.879770
37.023361	1402.215221	17.884787
37.068100	1408.425549	17.889805
37.532039	1415.364092	17.894823
37.314443	1411.271950	17.899840
37.424455	1399.502058	17.904858
37.220238	1406.678004	17.909875
37.613362	1407.179549	17.914893
37.489221	1404.849073	17.919911
37.204962	1402.046299	17.924928
37.492361	1412.369928	17.929946
37.396810	1418.011372	17.934963
37.475080	1430.123553	17.939981
37.497385	1434.324642	17.944999
37.253216	1433.857713	17.950016
37.739884	1427.385990	17.955034
37.591069	1428.033965	17.960051
37.799891	1432.530935	17.965069
37.904227	1427.768168	17.970087
37.608682	1431.232921	17.975104
38.080749	1428.726948	17.980122
38.034629	1438.799525	17.985139
38.002882	1424.227140	17.990157
38.278630	1420.346215	17.995175
37.955547	1432.083917	18.000192
38.213992	1421.289416	18.005210
37.830973	1422.211995	18.010227
37.939710	1423.206294	18.015245
38.242554	1426.057796	18.020263
37.970492	1426.437206	18.025280
38.237985	1425.508000	18.030298
38.029935	1424.791000	18.035315
38.331355	1423.111305	18.040333
38.379911	1420.351055	18.045351
38.451080	1419.330344	18.050368
38.301281	1422.104435	18.055386
38.402493	1424.623975	18.060403
38.191148	1424.439796	18.065421
38.272539	1430.549183	18.070439
38.622297	1455.346971	18.075456
38.883643	1452.581796	18.080474
38.587589	1448.849875	18.085491
38.587432	1452.997209	18.090509
38.747305	1449.150424	18.095527
38.745956	1454.147551	18.100544
38.749897	1449.854545	18.105562
38.612517	1454.838764	18.110579
38.572305	1460.100592	18.115597
38.774900	1449.504294	18.120615
38.563444	1458.725532	18.125632
38.763744	1448.101662	18.130650
39.040237	1449.148499	18.135667
38.955393	1469.149042	18.140685
39.119306	1474.472743	18.145703
38.884898	1472.274688	18.150720
39.231004	1470.112397	18.155738
39.088607	1470.909309	18.160755
39.121052	1471.535146	18.165773
39.318662	1477.412318	18.170791
39.220401	1472.822452	18.175808
39.561191	1473.299201	18.180826
39.489979	1466.593464	18.185843
39.484520	1469.216894	18.190861
39.634660	1468.647665	18.195879
39.675458	1467.448910	18.200896
39.865808	1463.939198	18.205914
39.636205	1472.299679	18.210931
39.276746	1471.608928	18.215949
39.855851	1466.221477	18.220967
39.620156	1472.344804	18.225984
39.654271	1472.032579	18.231002
39.923136	1464.567783	18.236019
39.802632	1466.599639	18.241037
39.652445	1468.686015	18.246055
39.671763	1470.723066	18.251072
39.846073	1468.578592	18.256090
39.659935	1469.701641	18.261107
39.694520	1460.713059	18.266125
40.010188	1479.503609	18.271143
39.910963	1500.266802	18.276160
40.109662	1497.169081	18.281178
40.230416	1502.258603	18.286195
39.826828	1505.985748	18.291213
40.095257	1501.094213	18.296231
40.132507	1504.953086	18.301248
40.303511	1496.348977	18.306266
40.165821	1497.020703	18.311283
40.101497	1499.629869	18.316301
40.327090	1501.022143	18.321319
40.336797	1493.410484	18.326336
40.385555	1501.496938	18.331354
40.299840	1518.356378	18.336371
40.445654	1528.804315	18.341389
40.493285	1525.854044	18.346407
40.460430	1530.163110	18.351424
40.719084	1522.879503	18.356442
40.593094	1520.479632	18.361459
40.876547	1525.958359	18.366477
40.985154	1523.648380	18.371495
40.977839	1524.623320	18.376512
40.849704	1528.977296	18.381530
41.137661	1517.119583	18.386547
40.938141	1516.534629	18.391565
40.990348	1518.120179	18.396583
40.863755	1519.182586	18.401600
41.215121	1525.303212	18.406618
41.108797	1518.592636	18.411635
41.155974	1528.437226	18.416653
41.222400	1512.940240	18.421671
41.303055	1527.814285	18.426688
41.731054	1536.976141	18.431706
41.575719	1521.054453	18.436723
41.204479	1520.367620	18.441741
41.452745	1510.984574	18.446759
41.778526	1517.960607	18.451776
41.220705	1526.306962	18.456794
41.547151	1526.540421	18.461811
41.643390	1549.023268	18.466829
41.869613	1538.632051	18.471847
41.825463	1540.301669	18.476864
41.691509	1534.993684	18.481882
41.647993	1542.711189	18.486899
41.934509	1541.322924	18.491917
42.012555	1540.078233	18.496935
42.133386	1547.282703	18.501952
42.070025	1544.608680	18.506970
41.871905	1546.680563	18.511987
42.038735	1551.729794	18.517005
42.136107	1547.009875	18.522023
41.864428	1554.125406	18.527040
41.771482	1546.896858	18.532058
41.894436	1542.919551	18.537075
41.851593	1541.653538	18.542093
41.491630	1550.320684	18.547111
41.551527	1560.645469	18.552128
42.053173	1567.817994	18.557146
42.450730	1572.134148	18.562163
42.305767	1576.496436	18.567181
42.708836	1578.833342	18.572199
42.599505	1574.129138	18.577216
42.619009	1570.468164	18.582234
42.464070	1568.282133	18.587251
42.102901	1580.368377	18.592269
42.643338	1564.449151	18.597287
42.670445	1572.845131	18.602304
42.467236	1577.847770	18.607322
42.751015	1595.261857	18.612339
42.484138	1604.977396	18.617357
42.603821	1606.276980	18.622375
42.755052	1614.253218	18.627392
43.031041	1601.737974	18.632410
43.330759	1597.870753	18.637427
43.040987	1611.052282	18.642445
43.038734	1602.764598	18.647463
42.995012	1599.644007	18.652480
42.805265	1607.186152	18.657498
42.855982	1597.969229	18.662515
42.949074	1610.247600	18.667533
43.126989	1618.893042	18.672551
43.207840	1626.143146	18.677568
43.234347	1623.979030	18.682586
43.423042	1616.930192	18.687603
43.442412	1627.808975	18.692621
43.952758	1623.082069	18.697639
44.000427	1628.042001	18.702656
43.644862	1627.808865	18.707674
43.994892	1619.077407	18.712691
43.568858	1630.357503	18.717709
43.644623	1620.782088	18.722727
43.815237	1624.562608	18.727744
44.175269	1616.288551	18.732762
44.404734	1616.601456	18.737779
43.922654	1622.000284	18.742797
44.076999	1619.525632	18.747815
44.074845	1617.459176	18.752832
43.892320	1617.881639	18.757850
43.971170	1612.871854	18.762867
43.914001	1618.336543	18.767885
44.112480	1615.578993	18.772903
44.237688	1612.012318	18.777920
44.256209	1617.170380	18.782938
44.537825	1613.017177	18.787955
44.108451	1615.655706	18.792973
44.170828	1614.578171	18.797991
44.596036	1618.424800	18.803008
44.048750	1616.846640	18.808026
44.203779	1617.478563	18.813043
43.890626	1625.941150	18.818061
44.571780	1636.405241	18.823079
44.736946	1642.068162	18.828096
44.383806	1647.397618	18.833114
44.807596	1643.198031	18.838131
44.654704	1646.826611	18.843149
44.884835	1649.953975	18.848167
45.073064	1647.436700	18.853184
44.841368	1647.807462	18.858202
44.620796	1637.695673	18.863219
45.185893	1643.365995	18.868237
45.028154	1642.231992	18.873255
45.033798	1635.677235	18.878272
44.985938	1643.286060	18.883290
45.548494	1636.877670	18.888307
44.839519	1641.334548	18.893325
44.738565	1644.325001	18.898343
45.091363	1655.935602	18.903360
45.129879	1670.940383	18.908378
45.336677	1664.182227	18.913395
45.170040	1669.202068	18.918413
45.480702	1666.281445	18.923431
45.482996	1670.538273	18.928448
45.112443	1674.212744	18.933466
45.291004	1663.405319	18.938483
45.345304	1672.973624	18.943501
45.898655	1695.488080	18.948519
45.804688	1696.811238	18.953536
46.150331	1695.690336	18.958554
46.037447	1681.390594	18.963571
45.871480	1669.783124	18.968589
45.687557	1658.619975	18.973607
46.026114	1670.465229	18.978624
45.919427	1684.689341	18.983642
46.124218	1678.106315	18.988659
46.457191	1690.766684	18.993677
46.423324	1679.721587	18.998695
46.271598	1659.599149	19.003712
46.455918	1653.766374	19.008730
46.518010	1662.680233	19.013747
46.404548	1650.849515	19.018765
46.328575	1648.803153	19.023783
46.475034	1652.545947	19.028800
45.563719	1658.998540	19.033818
46.556082	1666.595764	19.038835
46.466614	1679.580010	19.043853
46.260601	1687.867802	19.048871
46.714404	1684.715993	19.053888
46.707170	1694.168909	19.058906
46.388293	1686.446996	19.063923
46.493625	1683.687535	19.068941
46.974322	1688.533265	19.073959
46.940023	1680.054389	19.078976
46.722652	1687.071617	19.083994
46.790038	1692.743662	19.089011
46.726208	1710.529611	19.094029
47.247905	1716.018170	19.099047
47.017351	1715.291101	19.104064
46.771239	1719.978447	19.109082
46.920290	1716.290476	19.114099
46.908798	1712.442869	19.119117
46.852818	1716.742036	19.124135
47.023023	1723.695498	19.129152
46.979443	1746.800606	19.134170
47.379222	1738.847858	19.139187
47.252986	1746.689398	19.144205
46.975957	1747.881454	19.149223
47.576663	1742.301356	19.154240
47.496855	1740.011520	19.159258
47.914738	1732.029793	19.164275
48.094777	1736.190671	19.169293
47.833758	1733.195011	19.174311
47.910829	1724.191761	19.179328
48.203174	1732.465955	19.184346
47.963033	1730.651097	19.189363
48.108435	1733.450380	19.194381
47.748836	1736.767537	19.199399
47.988033	1731.900850	19.204416
48.154292	1735.275423	19.209434
48.137392	1738.665758	19.214451
48.071315	1747.113089	19.219469
48.162632	1755.713498	19.224487
48.464249	1753.443180	19.229504
48.392000	1754.673770	19.234522
48.470790	1765.369187	19.239539
48.697725	1764.109274	19.244557
48.579004	1756.420326	19.249575
48.347864	1754.348460	19.254592
48.570767	1765.886951	19.259610
48.486116	1747.039918	19.264627
48.488346	1768.916599	19.269645
48.503388	1761.822039	19.274663
48.554974	1755.750967	19.279680
48.344403	1757.559583	19.284698
48.762637	1764.342466	19.289715
48.814632	1756.057923	19.294733
48.693454	1753.048945	19.299751
48.854154	1753.377571	19.304768
48.609910	1766.380431	19.309786
48.574135	1776.704666	19.314803
48.924287	1783.735053	19.319821
49.129716	1787.341737	19.324839
49.266513	1789.160555	19.329856
49.028287	1789.539882	19.334874
49.316028	1784.402933	19.339891
49.453110	1788.339047	19.344909
49.260488	1784.934803	19.349927
49.330729	1782.457516	19.354944
49.421172	1791.109271	19.359962
49.611653	1805.896498	19.364979
49.592365	1815.772355	19.369997
49.582853	1818.163441	19.375015
49.796755	1820.083670	19.380032
49.672173	1822.230422	19.385050
49.829867	1818.194929	19.390067
49.618878	1819.042587	19.395085
49.521164	1811.702105	19.400103
49.593207	1812.549748	19.405120
49.590206	1814.953142	19.410138
49.905323	1823.455900	19.415155
50.226321	1831.013977	19.420173
50.017060	1839.118527	19.425191
50.402079	1839.839150	19.430208
50.017017	1839.673887	19.435226
50.464653	1839.189639	19.440243
50.700676	1840.730219	19.445261
50.502688	1843.223778	19.450279
50.606615	1844.509063	19.455296
50.355650	1848.257080	19.460314
50.024313	1837.100888	19.465331
50.569536	1838.819407	19.470349
50.329792	1842.452178	19.475367
51.018213	1836.528779	19.480384
50.730979	1840.747766	19.485402
50.562191	1838.823441	19.490419
50.799138	1842.787522	19.495437
50.853542	1861.122184	19.500455
51.273371	1864.858741	19.505472
51.165620	1859.026220	19.510490
50.752900	1846.601589	19.515507
50.916220	1858.894119	19.520525
50.952196	1867.872657	19.525543
51.172716	1863.273986	19.530560
51.083822	1864.234502	19.535578
51.320399	1866.212007	19.540595
51.190340	1861.044212	19.545613
51.039573	1867.816238	19.550631
51.445973	1854.625251	19.555648
51.273505	1861.779219	19.560666
51.707137	1872.004925	19.565683
51.634334	1875.985657	19.570701
51.695604	1896.660598	19.575719
51.924958	1886.325325	19.580736
52.206098	1885.461551	19.585754
51.925741	1868.106642	19.590771
51.692246	1871.506491	19.595789
51.780239	1873.359386	19.600807
52.197563	1880.576730	19.605824
52.300770	1888.371294	19.610842
52.197177	1874.006055	19.615859
52.114994	1854.282879	19.620877
51.914019	1857.157649	19.625895
52.357512	1875.066479	19.630912
52.073849	1882.155008	19.635930
52.213591	1881.107952	19.640947
52.448931	1888.466852	19.645965
52.476432	1892.446334	19.650983
52.483036	1883.163317	19.656000
51.980924	1889.247848	19.661018
51.906302	1892.478086	19.666035
52.136356	1894.781877	19.671053
52.018734	1898.169239	19.676071
52.271393	1904.774873	19.681088
52.263073	1911.731995	19.686106
52.509837	1919.622492	19.691123
52.554848	1911.409496	19.696141
52.485583	1931.373408	19.701159
52.791196	1937.399410	19.706176
52.791564	1945.211031	19.711194
53.142332	1939.851387	19.716211
53.320559	1938.801891	19.721229
53.030703	1948.260813	19.726247
53.197531	1939.313051	19.731264
53.045471	1941.032864	19.736282
53.036218	1938.888799	19.741299
53.016060	1944.347474	19.746317
53.270970	1965.068791	19.751335
53.403293	1951.688454	19.756352
53.520250	1972.741291	19.761370
53.279672	1962.337714	19.766387
53.742401	1954.291361	19.771405
54.141321	1969.648968	19.776423
53.852060	1957.495150	19.781440
53.748140	1962.740924	19.786458
53.916130	1962.865194	19.791475
54.222908	1955.658459	19.796493
53.741508	1960.621848	19.801511
54.210792	1957.302852	19.806528
54.232155	1952.738707	19.811546
53.973321	1962.666132	19.816563
54.178955	1954.820620	19.821581
54.133105	1964.795853	19.826599
54.223649	1973.618169	19.831616
54.191444	1983.947068	19.836634
54.396851	1997.155988	19.841651
54.763681	1992.316512	19.846669
54.366403	1990.891036	19.851687
54.845685	1985.488442	19.856704
54.475205	1986.152670	19.861722
54.717310	1983.266176	19.866739
55.069395	1978.146857	19.871757
54.554148	1981.182351	19.876775
54.826931	1977.374223	19.881792
54.781228	1982.030037	19.886810
54.811974	1982.366800	19.891827
55.075282	1976.349169	19.896845
54.568117	1979.882547	19.901863
55.246388	1982.035362	19.906880
55.262282	2000.414755	19.911898
55.343746	2006.427504	19.916915
55.380679	2005.992359	19.921933
55.426370	2007.581008	19.926951
55.628164	2003.964160	19.931968
55.420740	1997.485870	19.936986
55.141068	2014.768523	19.942003
55.420069	1998.038190	19.947021
55.154929	2005.091423	19.952039
55.477368	2001.879019	19.957056
55.564420	2009.620412	19.962074
55.338905	2012.391790	19.967091
55.567963	2006.336118	19.972109
55.680072	2022.310572	19.977127
55.572616	2032.274001	19.982144
55.833833	2043.763440	19.987162
56.136096	2039.898840	19.992179
56.277237	2034.827817	19.997197
55.940059	2040.787455	20.002215
56.115146	2044.180714	20.007232
55.957121	2034.862266	20.012250
55.683328	2038.137718	20.017267
56.134246	2037.165902	20.022285
56.269857	2059.269731	20.027303
56.492609	2060.221571	20.032320
56.358641	2062.242740	20.037338
56.531326	2065.454112	20.042355
56.632026	2060.800812	20.047373
56.713390	2064.097779	20.052391
56.813118	2064.105003	20.057408
56.937649	2064.126230	20.062426
56.848069	2056.882713	20.067443
56.945131	2045.952688	20.072461
56.839914	2055.390551	20.077479
56.941093	2058.616124	20.082496
56.927366	2060.383519	20.087514
56.871252	2072.528296	20.092531
57.260236	2083.196980	20.097549
57.511933	2090.952492	20.102567
57.514921	2087.467365	20.107584
57.512456	2088.101763	20.112602
57.642246	2097.362152	20.117619
57.825502	2087.107610	20.122637
57.745960	2089.823728	20.127655
57.840452	2073.230561	20.132672
57.666789	2064.980856	20.137690
57.802127	2078.262472	20.142707
58.168496	2073.812823	20.147725
57.972690	2062.153305	20.152743
57.600459	2057.177516	20.157760
57.991259	2059.361406	20.162778
57.593285	2083.193823	20.167795
58.068609	2081.890788	20.172813
58.243145	2081.980116	20.177831
57.909076	2084.816726	20.182848
58.140623	2081.685893	20.187866
58.063172	2081.870883	20.192883
58.417099	2079.706429	20.197901
58.153386	2090.324526	20.202919
58.160622	2076.579350	20.207936
58.543764	2096.742193	20.212954
58.454231	2104.400272	20.217971
58.699088	2099.582535	20.222989
58.833549	2097.944195	20.228007
58.769995	2106.066884	20.233024
58.747264	2096.623632	20.238042
58.699136	2101.128697	20.243059
58.447499	2099.822012	20.248077
58.431536	2097.968022	20.253095
58.432039	2107.487626	20.258112
59.002834	2121.481846	20.263130
58.791127	2131.044870	20.268147
59.093446	2135.388766	20.273165
59.229085	2131.646224	20.278183
59.313396	2129.842952	20.283200
59.036642	2128.038439	20.288218
59.029215	2142.563866	20.293235
59.507162	2151.630808	20.298253
59.582386	2155.630410	20.303271
59.576234	2154.205511	20.308288
59.618297	2148.865808	20.313306
59.618690	2157.277945	20.318323
59.829249	2158.867658	20.323341
59.878220	2156.763924	20.328359
60.074309	2155.743741	20.333376
60.608805	2152.098149	20.338394
60.005576	2155.548256	20.343411
59.938963	2148.869810	20.348429
60.081551	2151.168437	20.353447
60.123540	2151.359243	20.358464
59.991361	2143.337674	20.363482
59.641103	2149.987336	20.368499
59.687792	2156.120867	20.373517
60.061483	2172.445877	20.378535
60.248025	2175.058107	20.383552
60.344113	2171.342971	20.388570
60.332098	2176.569663	20.393587
60.767849	2180.754072	20.398605
61.079290	2202.505752	20.403623
60.776070	2193.321490	20.408640
60.929468	2198.360164	20.413658
60.728121	2198.595987	20.418675
61.201380	2201.391464	20.423693
61.179455	2198.692355	20.428711
61.283847	2195.778230	20.433728
61.527160	2198.085777	20.438746
61.544025	2203.843936	20.443763
61.575992	2195.641218	20.448781
61.509935	2181.110026	20.453799
61.147041	2176.312579	20.458816
61.329729	2178.073844	20.463834
61.623419	2191.993140	20.468851
61.443347	2198.227622	20.473869
61.976893	2197.941747	20.478887
61.609604	2195.658892	20.483904
62.040026	2193.903031	20.488922
61.787449	2193.057139	20.493939
61.761722	2185.604164	20.498957
61.797278	2193.311260	20.503975
61.882408	2202.058222	20.508992
62.081939	2192.321801	20.514010
61.771672	2198.911711	20.519027
61.942258	2203.399096	20.524045
62.237607	2218.311091	20.529063
62.265589	2217.102196	20.534080
62.139263	2221.239916	20.539098
62.178358	2219.762635	20.544115
62.413576	2223.503470	20.549133
62.486401	2219.988639	20.554151
62.107127	2219.294832	20.559168
62.439898	2229.124862	20.564186
62.684090	2253.361858	20.569203
62.896158	2252.033893	20.574221
62.847728	2250.939621	20.579239
63.052024	2260.432268	20.584256
63.089482	2254.106638	20.589274
63.049439	2253.049561	20.594291
63.291168	2252.662785	20.599309
63.345489	2249.145893	20.604327
63.172802	2247.691865	20.609344
63.400650	2244.122619	20.614362
63.437803	2252.597227	20.619379
63.176613	2255.240691	20.624397
63.407253	2252.537550	20.629415
63.405907	2248.927903	20.634432
63.569811	2258.763077	20.639450
63.367873	2279.325410	20.644467
64.040274	2278.636605	20.649485
64.126939	2278.368422	20.654503
63.538723	2272.116067	20.659520
63.980312	2268.742142	20.664538
63.849909	2275.868073	20.669555
63.821641	2275.133073	20.674573
63.672763	2276.159060	20.679591
63.510241	2277.146360	20.684608
64.192882	2288.027991	20.689626
64.093732	2294.640073	20.694643
63.929201	2295.165876	20.699661
64.527984	2291.954902	20.704679
64.384933	2295.621769	20.709696
64.712088	2291.026971	20.714714
64.731955	2288.412663	20.719731
64.709806	2292.107149	20.724749
64.775443	2289.925832	20.729767
64.997465	2289.131672	20.734784
64.998474	2281.952975	20.739802
65.351213	2291.169871	20.744819
64.926778	2292.617485	20.749837
65.359486	2281.037600	20.754855
65.058079	2285.344882	20.759872
65.190139	2282.254499	20.764890
65.098768	2284.406838	20.769907
65.052991	2286.302012	20.774925
65.258880	2305.810984	20.779943
65.081347	2323.168015	20.784960
65.543386	2316.535827	20.789978
65.639830	2309.417697	20.794995
65.707809	2325.992710	20.800013
65.823058	2311.411295	20.805031
65.753537	2324.111268	20.810048
65.761918	2328.704684	20.815066
65.738755	2316.409669	20.820083
65.801795	2323.580367	20.825101
66.168025	2335.937321	20.830119
65.999282	2339.019055	20.835136
65.882837	2350.166118	20.840154
65.971048	2348.831093	20.845171
66.017500	2349.909786	20.850189
66.052437	2343.262081	20.855207
65.895930	2352.339308	20.860224
66.270124	2365.057581	20.865242
66.157421	2375.951275	20.870259
66.251116	2371.087615	20.875277
66.565955	2375.599199	20.880295
66.499257	2381.789784	20.885312
66.735186	2390.517001	20.890330
67.168637	2398.529200	20.895347
66.832116	2403.142738	20.900365
67.458297	2393.803681	20.905383
67.025606	2399.148136	20.910400
67.342805	2399.767808	20.915418
67.287924	2400.799106	20.920435
67.261314	2392.770953	20.925453
67.567512	2396.994590	20.930471
67.305318	2398.281878	20.935488
67.618845	2390.126931	20.940506
67.881554	2394.924331	20.945523
67.679047	2398.178998	20.950541
67.956404	2391.298211	20.955559
67.684679	2400.969768	20.960576
67.524375	2389.350978	20.965594
67.692225	2384.610082	20.970611
67.742470	2395.555553	20.975629
67.560730	2396.022001	20.980647
67.603693	2422.461976	20.985664
68.295717	2417.558290	20.990682
68.453105	2425.802050	20.995699
68.283680	2428.958722	21.000717
68.384691	2426.074642	21.005735
68.239982	2414.404824	21.010752
68.525350	2418.329145	21.015770
68.331841	2420.376755	21.020787
68.188330	2418.682435	21.025805
68.964704	2424.268458	21.030823
68.748710	2441.583562	21.035840
68.778693	2433.202298	21.040858
69.294282	2436.897550	21.045875
69.069413	2436.115170	21.050893
69.338626	2432.972913	21.055911
69.356989	2439.330154	21.060928
69.407206	2431.518011	21.065946
69.334038	2417.239362	21.070963
69.399263	2429.067461	21.075981
69.198706	2427.453849	21.080999
69.271039	2437.114525	21.086016
69.319908	2430.708190	21.091034
69.618226	2423.617214	21.096051
69.288961	2431.248608	21.101069
69.407361	2428.147465	21.106087
69.752615	2424.502830	21.111104
69.561530	2446.455388	21.116122
69.607978	2459.966627	21.121139
69.713729	2471.570713	21.126157
69.882756	2465.049187	21.131175
70.121589	2465.560179	21.136192
69.900093	2470.498409	21.141210
70.189303	2471.792440	21.146227
70.098043	2481.101865	21.151245
70.618585	2478.253828	21.156263
70.725725	2485.205083	21.161280
70.170668	2486.987745	21.166298
70.506505	2482.319009	21.171315
70.462463	2491.779685	21.176333
70.754030	2480.899438	21.181351
70.482886	2484.269036	21.186368
70.202694	2497.523745	21.191386
70.860389	2508.643928	21.196403
70.942556	2512.008972	21.201421
70.925997	2509.144739	21.206439
71.113315	2508.368914	21.211456
71.296965	2514.425968	21.216474
71.384888	2510.027026	21.221491
71.371070	2514.161155	21.226509
71.531218	2517.271936	21.231527
71.647217	2535.336943	21.236544
71.716275	2541.039732	21.241562
72.082709	2526.341718	21.246579
71.917216	2537.235998	21.251597
71.761363	2532.568341	21.256615
72.172914	2537.776205	21.261632
71.722952	2536.451135	21.266650
72.023936	2528.831294	21.271667
71.960470	2528.848216	21.276685
72.091991	2530.405384	21.281703
71.893528	2531.348647	21.286720
72.003663	2529.302062	21.291738
72.399175	2539.374672	21.296755
72.442422	2556.144587	21.301773
72.453036	2559.585666	21.306791
72.778817	2559.008185	21.311808
72.902306	2563.495205	21.316826
73.134928	2560.039671	21.321843
72.932359	2562.105335	21.326861
72.983994	2552.784147	21.331879
73.082860	2549.650385	21.336896
73.025838	2564.437189	21.341914
73.013201	2558.816621	21.346931
72.915953	2558.396197	21.351949
73.367681	2549.892674	21.356967
73.352986	2554.400603	21.361984
73.128352	2561.536361	21.367002
73.234991	2559.052137	21.372019
73.049557	2552.999132	21.377037
73.298070	2563.387059	21.382055
73.558360	2575.368414	21.387072
73.502303	2584.868934	21.392090
73.694427	2581.914619	21.397107
73.687747	2585.110914	21.402125
74.077355	2570.359413	21.407143
73.911296	2580.195879	21.412160
74.038741	2592.711873	21.417178
74.269065	2607.716510	21.422195
74.302026	2620.954515	21.427213
74.547447	2611.492536	21.432231
74.367188	2614.804198	21.437248
74.398485	2619.090737	21.442266
74.446929	2612.692666	21.447283
74.237494	2613.686572	21.452301
74.223106	2610.081363	21.457319
74.592687	2621.531634	21.462336
74.606533	2642.382751	21.467354
74.881789	2631.053103	21.472371
74.861749	2640.791015	21.477389
75.225876	2624.818407	21.482407
74.929940	2638.973537	21.487424
74.745489	2636.844604	21.492442
75.306752	2648.160001	21.497459
75.552387	2667.692376	21.502477
75.419120	2668.312233	21.507495
75.206592	2658.694933	21.512512
75.346409	2674.135120	21.517530
75.227193	2662.067168	21.522547
75.543026	2667.011379	21.527565
75.647486	2678.664655	21.532583
76.071261	2688.308639	21.537600
75.683106	2692.738670	21.542618
76.127787	2686.002896	21.547635
76.344510	2691.029671	21.552653
76.100718	2686.719464	21.557671
76.123129	2683.758189	21.562688
76.420600	2689.440142	21.567706
76.531219	2673.281492	21.572723
76.336603	2677.947602	21.577741
76.288270	2684.029352	21.582759
76.451631	2703.947861	21.587776
76.704775	2721.347812	21.592794
76.963917	2711.496073	21.597811
76.777860	2714.665005	21.602829
76.789969	2709.150136	21.607847
76.809291	2704.178207	21.612864
76.847162	2719.217179	21.617882
77.285851	2721.245590	21.622899
77.611636	2739.795426	21.627917
77.234455	2734.604079	21.632935
77.745846	2737.689033	21.637952
77.450926	2737.552138	21.642970
77.648889	2728.942888	21.647987
77.506875	2733.890877	21.653005
77.626212	2725.872640	21.658023
77.863725	2730.950715	21.663040
78.065204	2731.673427	21.668058
78.142148	2723.202730	21.673075
77.864935	2725.231953	21.678093
78.155747	2728.262083	21.683111
78.371132	2727.353245	21.688128
78.169233	2727.437579	21.693146
78.322460	2720.013776	21.698163
78.490548	2720.664846	21.703181
78.492293	2723.842451	21.708199
78.598581	2721.895304	21.713216
78.462799	2734.605007	21.718234
78.758038	2750.048671	21.723251
78.942467	2751.752230	21.728269
78.922005	2762.445868	21.733287
78.817915	2752.630622	21.738304
78.775177	2753.422120	21.743322
78.840298	2758.084227	21.748339
78.681516	2754.976942	21.753357
79.048374	2768.975987	21.758375
79.401565	2785.200699	21.763392
79.106416	2787.636472	21.768410
79.723095	2781.610422	21.773427
79.347419	2786.239609	21.778445
79.229061	2790.076531	21.783463
79.608851	2774.603970	21.788480
79.613964	2796.578475	21.793498
80.060368	2800.949100	21.798515
79.679893	2814.761667	21.803533
79.794798	2813.460769	21.808551
79.913156	2809.797704	21.813568
79.784632	2818.520148	21.818586
79.903326	2827.093781	21.823603
80.191957	2845.223090	21.828621
80.187451	2842.258760	21.833639
80.487910	2837.050067	21.838656
80.280566	2847.293567	21.843674
80.622769	2834.920324	21.848691
80.978908	2857.838051	21.853709
81.200366	2865.578879	21.858727
81.343770	2866.351374	21.863744
80.955443	2860.508235	21.868762
81.472267	2865.576723	21.873779
81.358027	2865.720566	21.878797
81.776193	2861.578287	21.883815
82.161691	2845.433005	21.888832
81.961524	2831.413212	21.893850
82.031572	2818.415307	21.898867
81.761918	2816.950506	21.903885
81.979208	2819.855416	21.908903
82.016089	2813.452877	21.913920
81.536529	2822.198403	21.918938
81.931865	2818.232764	21.923955
81.612695	2813.401498	21.928973
81.708014	2843.053839	21.933991
82.096066	2845.345002	21.939008
81.874323	2855.094002	21.944026
82.697382	2848.357719	21.949043
82.509064	2852.075520	21.954061
82.328104	2864.402227	21.959079
82.324437	2851.242865	21.964096
82.265351	2861.187789	21.969114
83.046958	2865.954149	21.974131
82.779144	2875.401317	21.979149
82.504722	2875.740592	21.984167
82.603227	2879.853070	21.989184
82.760295	2883.186500	21.994202
82.613892	2877.568280	21.999219
82.763825	2887.251035	22.004237
82.802396	2892.309342	22.009255
83.337466	2901.608233	22.014272
83.043826	2903.021644	22.019290
83.256689	2904.669327	22.024307
83.192522	2918.806808	22.029325
83.174291	2932.492959	22.034343
83.167659	2923.508389	22.039360
83.557323	2938.658631	22.044378
83.734661	2946.651706	22.049395
84.020277	2953.744893	22.054413
83.825134	2959.835310	22.059431
84.013868	2964.265970	22.064448
84.113700	2958.720739	22.069466
84.264136	2959.994479	22.074483
84.387612	2963.239780	22.079501
84.405704	2981.484127	22.084519
84.264600	2983.768429	22.089536
84.609008	2997.065824	22.094554
84.799758	2989.202179	22.099571
84.790514	2987.679676	22.104589
84.660991	2996.317731	22.109607
85.084136	2980.819676	22.114624
85.319532	2988.483842	22.119642
85.313319	2989.378368	22.124659
85.457076	2989.301919	22.129677
85.263477	3010.257567	22.134695
85.515727	3008.956749	22.139712
85.481922	3014.691311	22.144730
85.787757	3009.319058	22.149747
85.845739	3003.134227	22.154765
86.183456	3009.366377	22.159783
86.331629	3001.325113	22.164800
85.980547	3010.733783	22.169818
86.137652	3004.773111	22.174835
85.923184	3006.998691	22.179853
85.833295	3006.888480	22.184871
86.217214	3006.852195	22.189888
86.264607	3022.447019	22.194906
86.311335	3028.531276	22.199923
86.512019	3028.881660	22.204941
86.554120	3027.957005	22.209959
86.851890	3029.070518	22.214976
86.534924	3030.763417	22.219994
86.272836	3026.745540	22.225011
86.795774	3037.234423	22.230029
86.498691	3056.283078	22.235047
87.127084	3055.175906	22.240064
87.052404	3056.877909	22.245082
87.388770	3063.566644	22.250099
87.949355	3073.425246	22.255117
88.014025	3077.820570	22.260135
87.688030	3061.641281	22.265152
87.903156	3058.914192	22.270170
87.890500	3057.780865	22.275187
87.960290	3064.616898	22.280205
87.795043	3079.894592	22.285223
88.500601	3071.183393	22.290240
88.637331	3070.923444	22.295258
88.521091	3070.265183	22.300275
88.759145	3062.117266	22.305293
88.266773	3076.225386	22.310311
88.564593	3069.302329	22.315328
88.571926	3071.660500	22.320346
88.651157	3068.016454	22.325363
89.073872	3066.251934	22.330381
88.625127	3072.891911	22.335399
88.317189	3065.043074	22.340416
88.833531	3068.964755	22.345434
88.566474	3072.788567	22.350451
88.998392	3083.528795	22.355469
88.608150	3103.505221	22.360487
89.163974	3095.090085	22.365504
89.113086	3097.389784	22.370522
89.091956	3110.370205	22.375539
89.465989	3125.324380	22.380557
89.101396	3128.743448	22.385575
89.493529	3128.382544	22.390592
89.419634	3130.169078	22.395610
89.450540	3153.855334	22.400627
89.844622	3154.367026	22.405645
89.699322	3146.749118	22.410663
89.990358	3156.800449	22.415680
90.440430	3177.963950	22.420698
90.608328	3179.557685	22.425715
91.058062	3170.323378	22.430733
90.913641	3172.526358	22.435751
91.057328	3176.706639	22.440768
91.096435	3174.902069	22.445786
91.158156	3168.470860	22.450803
91.330962	3164.223445	22.455821
90.958823	3157.399464	22.460839
91.498047	3166.816737	22.465856
91.645332	3163.314959	22.470874
91.378633	3174.557180	22.475891
91.669492	3170.540241	22.480909
91.423972	3178.374293	22.485927
91.416196	3176.857434	22.490944
91.918787	3160.199480	22.495962
91.496025	3171.756149	22.500979
91.377418	3167.989702	22.505997
91.570923	3170.302889	22.511015
91.825350	3188.343370	22.516032
91.877336	3195.069799	22.521050
91.870479	3198.214669	22.526067
92.375011	3198.058405	22.531085
92.209334	3203.147480	22.536103
92.123515	3218.535793	22.541120
92.398035	3226.529853	22.546138
92.324964	3226.746023	22.551155
92.817285	3228.521110	22.556173
92.536214	3233.491886	22.561191
92.663739	3244.951984	22.566208
92.786368	3252.040795	22.571226
92.961984	3253.735238	22.576243
93.275449	3251.801760	22.581261
92.651464	3267.399711	22.586279
93.451627	3266.435364	22.591296
93.593814	3274.802577	22.596314
93.456142	3278.886147	22.601331
93.712001	3277.872536	22.606349
93.643806	3275.161608	22.611367
93.824034	3274.012079	22.616384
93.933033	3276.577488	22.621402
93.643118	3296.539123	22.626419
94.075748	3298.571766	22.631437
94.037390	3310.247586	22.636455
93.892864	3310.057434	22.641472
94.459168	3309.689738	22.646490
94.474271	3331.508994	22.651507
94.877521	3319.741077	22.656525
94.702361	3330.271327	22.661543
94.612940	3333.906717	22.666560
95.143434	3326.932817	22.671578
95.014385	3334.840586	22.676595
95.472412	3328.993371	22.681613
95.424675	3322.691258	22.686631
95.296429	3318.865341	22.691648
95.172906	3326.685961	22.696666
94.983450	3325.094827	22.701683
95.333334	3332.999290	22.706701
95.406554	3343.246271	22.711719
95.720113	3351.374892	22.716736
95.705972	3348.347881	22.721754
95.958370	3357.361924	22.726771
95.996079	3343.017608	22.731789
96.173711	3350.585993	22.736807
96.024125	3360.927363	22.741824
96.095608	3373.807226	22.746842
96.372724	3380.746881	22.751859
96.603119	3372.109859	22.756877
96.434921	3377.188778	22.761895
96.318566	3380.520337	22.766912
96.730313	3383.611685	22.771930
96.753430	3400.300004	22.776947
96.914759	3397.516008	22.781965
97.431915	3398.968465	22.786983
96.960737	3402.278059	22.792000
97.106987	3388.242146	22.797018
96.568872	3402.781801	22.802035
97.593327	3419.263397	22.807053
97.459089	3432.799883	22.812071
97.916705	3436.827063	22.817088
97.915527	3424.994517	22.822106
98.052644	3430.532802	22.827123
97.891748	3433.787092	22.832141
98.171903	3428.795370	22.837159
98.085642	3427.322982	22.842176
98.245258	3432.553177	22.847194
98.447344	3454.702317	22.852211
98.718466	3461.487077	22.857229
98.462090	3460.258625	22.862247
98.779613	3458.884358	22.867264
99.202223	3453.811162	22.872282
99.127935	3455.229251	22.877299
99.421742	3447.721585	22.882317
99.245484	3447.798132	22.887335
99.302345	3446.822971	22.892352
99.260486	3450.735587	22.897370
99.229162	3441.234668	22.902387
99.314699	3437.922601	22.907405
99.239839	3450.087696	22.912423
99.584759	3469.032524	22.917440
100.055806	3469.610235	22.922458
99.614718	3473.846467	22.927475
99.829876	3468.863526	22.932493
100.349247	3476.535646	22.937511
99.888809	3482.042950	22.942528
100.220758	3475.705866	22.947546
99.842066	3485.793485	22.952563
100.362456	3493.196515	22.957581
100.327883	3508.058455	22.962599
100.343359	3505.411596	22.967616
100.656708	3504.629820	22.972634
100.573024	3515.504146	22.977651
100.747173	3530.907604	22.982669
101.190969	3529.436431	22.987687
100.572043	3531.907811	22.992704
100.999448	3533.280248	22.997722
100.903718	3542.007901	23.002739
101.545829	3551.430818	23.007757
101.857094	3556.040597	23.012775
101.486704	3561.829513	23.017792
101.898584	3548.164487	23.022810
101.923851	3554.266677	23.027827
101.995363	3554.360082	23.032845
102.131868	3551.906982	23.037863
101.881920	3562.921088	23.042880
102.138750	3553.125117	23.047898
102.138098	3572.044993	23.052915
102.391831	3575.228693	23.057933
102.592309	3574.325821	23.062951
102.684731	3583.530676	23.067968
102.655502	3584.559772	23.072986
102.538299	3584.389504	23.078003
102.480401	3580.094731	23.083021
102.801794	3589.123079	23.088039
102.691058	3609.750020	23.093056
103.147878	3609.905630	23.098074
102.771440	3623.259912	23.103091
103.009422	3630.868053	23.108109
102.927124	3633.903832	23.113127
103.255989	3644.996593	23.118144
103.427719	3645.585283	23.123162
103.585025	3673.127091	23.128179
103.669103	3674.578436	23.133197
104.185986	3671.378784	23.138215
103.717479	3673.480354	23.143232
104.387396	3676.483342	23.148250
104.575948	3690.149700	23.153267
104.787298	3689.670274	23.158285
104.854154	3685.345761	23.163303
104.978623	3698.902248	23.168320
105.305287	3687.201863	23.173338
105.183486	3686.664984	23.178355
105.161808	3684.539274	23.183373
105.444616	3688.932122	23.188391
105.140585	3685.951861	23.193408
105.297783	3686.889854	23.198426
105.488160	3678.986944	23.203443
105.477528	3673.510939	23.208461
105.605664	3673.862327	23.213479
104.982406	3694.345861	23.218496
105.661241	3710.616454	23.223514
105.712823	3702.663669	23.228531
105.755319	3712.620271	23.233549
105.929963	3717.721679	23.238567
106.002718	3743.660073	23.243584
106.059125	3736.365222	23.248602
106.230340	3747.617640	23.253619
106.325775	3751.624150	23.258637
106.837916	3771.875304	23.263655
106.549023	3781.013076	23.268672
107.007466	3770.439000	23.273690
106.891777	3764.465719	23.278707
107.039846	3764.257040	23.283725
107.293820	3778.878524	23.288743
107.178089	3783.485436	23.293760
107.602164	3782.917236	23.298778
107.730323	3789.611228	23.303795
107.769924	3781.008722	23.308813
107.820565	3773.207258	23.313831
107.796602	3786.016244	23.318848
107.976113	3780.558332	23.323866
108.043675	3795.882441	23.328883
108.159310	3811.034803	23.333901
108.345884	3811.449758	23.338919
108.255250	3821.055584	23.343936
108.477839	3810.886330	23.348954
108.426329	3814.437985	23.353971
108.321857	3818.557937	23.358989
108.845131	3832.149312	23.364007
108.841780	3842.092324	23.369024
109.153632	3845.834648	23.374042
109.056490	3841.078518	23.379059
109.505491	3837.810535	23.384077
109.319102	3833.459790	23.389095
109.243468	3845.834405	23.394112
109.270915	3837.798920	23.399130
109.521187	3854.211103	23.404147
109.532393	3868.232222	23.409165
109.643900	3874.024941	23.414183
109.749529	3879.161060	23.419200
109.937785	3876.711942	23.424218
110.316779	3888.683712	23.429235
110.323569	3889.635988	23.434253
110.840943	3884.767470	23.439271
110.641689	3889.389423	23.444288
110.749882	3889.368080	23.449306
110.938808	3891.640789	23.454323
110.807650	3877.229835	23.459341
111.057646	3879.719629	23.464359
111.123280	3885.217935	23.469376
111.326128	3899.545197	23.474394
111.233147	3904.737046	23.479411
111.309436	3909.072798	23.484429
111.906021	3904.666425	23.489447
111.610167	3913.501838	23.494464
111.635286	3907.400056	23.499482
112.083075	3905.660435	23.504499
111.772598	3917.209689	23.509517
112.205322	3919.171526	23.514535
112.006726	3931.399218	23.519552
112.351264	3937.259693	23.524570
112.391028	3945.621386	23.529587
112.066727	3947.198253	23.534605
112.761055	3945.776129	23.539623
112.507398	3977.685182	23.544640
112.409603	3967.859073	23.549658
112.761708	3971.180134	23.554675
112.776074	3985.832819	23.559693
113.221578	3990.109433	23.564711
113.085907	3997.830807	23.569728
113.351701	3994.875451	23.574746
113.133445	3998.005081	23.579763
113.591595	4018.501751	23.584781
114.140787	4016.115312	23.589799
114.268655	4027.083333	23.594816
114.320298	4016.171659	23.599834
114.460948	4019.566329	23.604851
114.413403	4031.769090	23.609869
114.484414	4015.099000	23.614887
114.768640	4010.037120	23.619904
115.061760	4003.293200	23.624922
115.337189	4004.230538	23.629939
114.987506	4005.372964	23.634957
115.041014	4005.661114	23.639975
115.251647	4005.012875	23.644992
115.155550	4006.954388	23.650010
115.382459	4005.231639	23.655027
115.173258	4027.149246	23.660045
115.219119	4029.461019	23.665063
115.142775	4032.071809	23.670080
115.263022	4046.301447	23.675098
115.739241	4053.451389	23.680115
115.897435	4069.150583	23.685133
116.098252	4063.934754	23.690151
115.692885	4061.792979	23.695168
116.173232	4074.166680	23.700186
116.462790	4081.746815	23.705203
116.466088	4087.354347	23.710221
116.710816	4089.871824	23.715239
116.445333	4092.518663	23.720256
116.357535	4089.533630	23.725274
116.878038	4105.769032	23.730291
116.785102	4117.899835	23.735309
117.045315	4117.355212	23.740327
117.220558	4122.840573	23.745344
117.459197	4115.462217	23.750362
117.760956	4136.751986	23.755379
117.762760	4139.842059	23.760397
117.847521	4144.413126	23.765415
117.835852	4145.923287	23.770432
117.632375	4153.424431	23.775450
118.108765	4142.797521	23.780467
118.084681	4150.050817	23.785485
118.298986	4162.649768	23.790503
118.494947	4168.621557	23.795520
118.295533	4180.484165	23.800538
118.719385	4168.185349	23.805555
118.319683	4171.474996	23.810573
118.790423	4182.798235	23.815591
118.656602	4192.172424	23.820608
118.951770	4190.940798	23.825626
119.149845	4204.547358	23.830643
119.270763	4220.950628	23.835661
119.434669	4221.306345	23.840679
119.747882	4221.423134	23.845696
120.186521	4218.280038	23.850714
120.130630	4206.472500	23.855731
120.060856	4224.304426	23.860749
120.477846	4228.784285	23.865767
120.542242	4237.439742	23.870784
120.668429	4236.936994	23.875802
121.051480	4225.270189	23.880819
120.564843	4240.425815	23.885837
120.743684	4236.960315	23.890855
121.049552	4235.140990	23.895872
120.916014	4235.797176	23.900890
120.931567	4237.816311	23.905907
120.802365	4258.675153	23.910925
120.940555	4263.892636	23.915943
121.539116	4265.470309	23.920960
121.331808	4276.857838	23.925978
121.911999	4288.421345	23.930995
121.875129	4292.735380	23.936013
122.380548	4292.647089	23.941031
122.312822	4293.351447	23.946048
122.144834	4302.215522	23.951066
122.074982	4291.478130	23.956083
122.183571	4313.179713	23.961101
122.320751	4311.322155	23.966119
122.530929	4317.116028	23.971136
122.893814	4324.534509	23.976154
123.063576	4323.035397	23.981171
122.809841	4343.564516	23.986189
123.048902	4350.857816	23.991207
123.306388	4353.503167	23.996224
123.345785	4353.500696	24.001242
123.541886	4358.630656	24.006259
123.887571	4375.857655	24.011277
124.153662	4378.215709	24.016295
124.171930	4370.703611	24.021312
124.337668	4381.678210	24.026330
124.439307	4374.388569	24.031347
124.441281	4369.570191	24.036365
124.529465	4373.103569	24.041383
124.483686	4371.789771	24.046400
124.282313	4380.554675	24.051418
124.595245	4375.372946	24.056435
124.528339	4399.376543	24.061453
124.759595	4405.749739	24.066471
124.924523	4402.652712	24.071488
124.845368	4414.616079	24.076506
125.127694	4419.152941	24.081523
125.066275	4434.205276	24.086541
125.404326	4437.822518	24.091559
125.510487	4443.124119	24.096576
125.646175	4455.644179	24.101594
125.806568	4451.452421	24.106611
126.004567	4470.605105	24.111629
126.422460	4475.969299	24.116647
126.662434	4486.030730	24.121664
126.612017	4490.150964	24.126682
127.089902	4486.220074	24.131699
126.819986	4485.358412	24.136717
126.940881	4488.739130	24.141735
127.331359	4487.194797	24.146752
127.092473	4487.768418	24.151770
127.283156	4470.195980	24.156787
127.462835	4485.233648	24.161805
127.291259	4501.439924	24.166823
127.393012	4492.066364	24.171840
127.718268	4502.327111	24.176858
127.720852	4510.610205	24.181875
127.918596	4531.746835	24.186893
128.058637	4533.211440	24.191911
128.016020	4523.281341	24.196928
128.128845	4537.931629	24.201946
128.582202	4545.035181	24.206963
128.485577	4550.953177	24.211981
128.587206	4561.530567	24.216999
128.737927	4557.653039	24.222016
129.028755	4579.599673	24.227034
129.321961	4577.543779	24.232051
129.878746	4582.220323	24.237069
129.725230	4579.665840	24.242087
129.724176	4571.466164	24.247104
129.869417	4584.180057	24.252122
130.068095	4566.929872	24.257139
130.048307	4578.828406	24.262157
129.688066	4598.790341	24.267175
130.163661	4591.011046	24.272192
129.881127	4599.060237	24.277210
129.929424	4606.931800	24.282227
130.250939	4627.012437	24.287245
130.573523	4629.536801	24.292263
131.502626	4647.689750	24.297280
131.100070	4655.576128	24.302298
131.540834	4647.982922	24.307315
131.643682	4660.542448	24.312333
131.776068	4655.441710	24.317351
132.114538	4647.607123	24.322368
131.977857	4660.343340	24.327386
132.001510	4646.265960	24.332403
132.032968	4646.501857	24.337421
132.106856	4653.851784	24.342439
132.286958	4651.044380	24.347456
132.128584	4658.715495	24.352474
132.454635	4677.985842	24.357491
132.599553	4684.498667	24.362509
132.448623	4691.410150	24.367527
132.818962	4680.236550	24.372544
132.529727	4695.562330	24.377562
133.092122	4702.911733	24.382579
133.076435	4716.565155	24.387597
132.961019	4705.686174	24.392615
133.271485	4713.828621	24.397632
133.388624	4736.293303	24.402650
133.638950	4733.873549	24.407667
133.712864	4739.271946	24.412685
133.561487	4745.584196	24.417703
133.810506	4752.156206	24.422720
134.274534	4765.428613	24.427738
134.488808	4759.619658	24.432755
134.512436	4767.576505	24.437773
134.401559	4771.812355	24.442791
134.999929	4789.054678	24.447808
134.425383	4799.321257	24.452826
135.009476	4796.754877	24.457843
135.427415	4800.490501	24.462861
135.326141	4817.910120	24.467879
135.730852	4813.001302	24.472896
135.343867	4823.099020	24.477914
135.592541	4823.187123	24.482931
135.598385	4821.749757	24.487949
135.672094	4843.079817	24.492967
136.022023	4841.483098	24.497984
135.839093	4857.347455	24.503002
136.375132	4857.150925	24.508019
136.792759	4868.059748	24.513037
136.614172	4877.342522	24.518055
136.752623	4873.576420	24.523072
137.025180	4879.877603	24.528090
137.277851	4891.763556	24.533107
137.439514	4899.688165	24.538125
137.604125	4904.421861	24.543143
137.879520	4900.049493	24.548160
137.838637	4910.438070	24.553178
137.495665	4896.558202	24.558195
138.134559	4897.044789	24.563213
138.479909	4910.363744	24.568231
138.456221	4908.724917	24.573248
138.684339	4916.057309	24.578266
138.768875	4912.696269	24.583283
139.077741	4918.179476	24.588301
138.894642	4917.400286	24.593319
139.119778	4908.849534	24.598336
138.990093	4913.526423	24.603354
138.925142	4925.317712	24.608371
139.210696	4934.244877	24.613389
139.491891	4947.545346	24.618407
139.563828	4944.787300	24.623424
139.674558	4944.455629	24.628442
139.745678	4966.206059	24.633459
139.908563	4968.139465	24.638477
139.818593	4977.670674	24.643495
140.372531	4985.757202	24.648512
140.118534	4996.445742	24.653530
140.125404	5000.785807	24.658547
140.437925	5008.385431	24.663565
140.544918	5026.149621	24.668583
141.021395	5026.644989	24.673600
141.072998	5045.451665	24.678618
141.134641	5047.772002	24.683635
141.551859	5054.855781	24.688653
141.649534	5061.874331	24.693671
141.981472	5048.983617	24.698688
141.962553	5058.607859	24.703706
142.079564	5066.932158	24.708723
142.651606	5072.146601	24.713741
142.748637	5077.273512	24.718759
142.688458	5073.542610	24.723776
142.738788	5079.935009	24.728794
143.061253	5079.487948	24.733811
143.135516	5073.525642	24.738829
142.802799	5086.807369	24.743847
142.786049	5068.599170	24.748864
143.046105	5077.278615	24.753882
142.818069	5098.038369	24.758899
143.511556	5100.953473	24.763917
142.991295	5107.026873	24.768935
143.536530	5125.127371	24.773952
143.504710	5132.302855	24.778970
143.742156	5144.001713	24.783987
144.105616	5152.532554	24.789005
144.194520	5171.886873	24.794023
144.197569	5168.945662	24.799040
144.295055	5177.209457	24.804058
144.999753	5195.664037	24.809075
145.138545	5191.073994	24.814093
145.024909	5203.306720	24.819111
145.212529	5189.446646	24.824128
145.303083	5213.953094	24.829146
145.263803	5212.984685	24.834163
145.554921	5224.018662	24.839181
145.615966	5234.578809	24.844199
146.091608	5249.112986	24.849216
146.450724	5252.439465	24.854234
146.080052	5249.260829	24.859251
146.281037	5243.843751	24.864269
146.244100	5258.771532	24.869287
146.790253	5276.774393	24.874304
147.203617	5278.879016	24.879322
147.426284	5269.624378	24.884339
147.489136	5268.840679	24.889357
147.288566	5273.797188	24.894375
147.526486	5282.871840	24.899392
148.168975	5286.577495	24.904410
148.076205	5292.695177	24.909427
148.285223	5289.456790	24.914445
148.406022	5300.975031	24.919463
148.133272	5290.965197	24.924480
148.493066	5292.632131	24.929498
148.338911	5293.887975	24.934515
149.091567	5318.447211	24.939533
149.025048	5329.419971	24.944551
148.591089	5318.514545	24.949568
148.849889	5321.778889	24.954586
148.841701	5332.357652	24.959603
149.586601	5333.923028	24.964621
149.312061	5348.937487	24.969639
149.512354	5344.894830	24.974656
149.850564	5370.025243	24.979674
149.913331	5383.397686	24.984691
150.210267	5370.964582	24.989709
150.012660	5384.815670	24.994727
150.337134	5396.649163	24.999744
150.379468	5406.552522	25.004762
150.674295	5404.009524	25.009779
150.829689	5417.309166	25.014797
151.148144	5434.439450	25.019815
151.549956	5441.951256	25.024832
151.481758	5436.337674	25.029850
151.319188	5444.602134	25.034867
151.986921	5439.090389	25.039885
151.686378	5455.881337	25.044903
152.005494	5463.085506	25.049920
152.272085	5467.304729	25.054938
152.087022	5465.653181	25.059955
152.187109	5464.564022	25.064973
152.320079	5482.194472	25.069991
152.686559	5487.772304	25.075008
152.613159	5492.271499	25.080026
152.890438	5497.514410	25.085043
153.154988	5500.685691	25.090061
153.291234	5516.539609	25.095079
153.135508	5513.156788	25.100096
153.445959	5516.915895	25.105114
153.771337	5523.882777	25.110131
153.981461	5536.831642	25.115149
153.820440	5537.005695	25.120167
154.216521	5546.515847	25.125184
154.252584	5550.300700	25.130202
154.502217	5561.092113	25.135219
154.588899	5565.969652	25.140237
154.547343	5571.952948	25.145255
154.752959	5572.287617	25.150272
154.742783	5579.502251	25.155290
154.833328	5596.699585	25.160307
155.256439	5600.964603	25.165325
155.268760	5615.536446	25.170343
155.302309	5620.262128	25.175360
155.921596	5625.693404	25.180378
156.030257	5647.322781	25.185395
156.296434	5650.904164	25.190413
156.014056	5659.925768	25.195431
156.281653	5659.761864	25.200448
156.672732	5672.715537	25.205466
156.548434	5678.137620	25.210483
156.954543	5675.013019	25.215501
156.869649	5691.506242	25.220519
157.056229	5708.891001	25.225536
157.453878	5708.705565	25.230554
157.425493	5717.047190	25.235571
157.834099	5726.722351	25.240589
158.082007	5738.222230	25.245607
158.230268	5739.386298	25.250624
158.688035	5748.542177	25.255642
158.824718	5746.207245	25.260659
158.805043	5760.163096	25.265677
158.911097	5775.224425	25.270695
158.660315	5772.073877	25.275712
158.939528	5770.575415	25.280730
159.058253	5777.916081	25.285747
159.625569	5778.902873	25.290765
159.173677	5793.213061	25.295783
159.151432	5797.035192	25.300800
159.780491	5815.418752	25.305818
159.869354	5816.358739	25.310835
160.294824	5814.518651	25.315853
160.350347	5833.135803	25.320871
160.465974	5844.215021	25.325888
160.668195	5846.835912	25.330906
160.629303	5855.795263	25.335923
160.645448	5861.387122	25.340941
161.052934	5867.349745	25.345959
161.301660	5878.256518	25.350976
161.503288	5882.095952	25.355994
161.276480	5902.231979	25.361011
161.413313	5907.006807	25.366029
161.790513	5919.327375	25.371047
161.838233	5928.089700	25.376064
162.359385	5939.417683	25.381082
162.195360	5927.552720	25.386099
162.485214	5936.084361	25.391117
162.671879	5962.595510	25.396135
162.894751	5961.030746	25.401152
163.573671	5958.407533	25.406170
163.238910	5966.435344	25.411187
163.501170	5968.638329	25.416205
163.722297	5983.745391	25.421223
163.677712	5982.838459	25.426240
164.148892	5984.445285	25.431258
163.848937	5989.472028	25.436275
163.957938	5991.785452	25.441293
164.225534	6005.670332	25.446311
164.088117	6018.527482	25.451328
164.568107	6012.208595	25.456346
164.461972	6027.083972	25.461363
164.529380	6042.044049	25.466381
165.080914	6043.696651	25.471399
165.112442	6059.777171	25.476416
165.663754	6070.696205	25.481434
166.006332	6079.057732	25.486451
165.676976	6071.875680	25.491469
166.087967	6087.213687	25.496487
165.709354	6103.014022	25.501504
166.213731	6112.677504	25.506522
166.500866	6107.166320	25.511539
166.829635	6121.468855	25.516557
166.926998	6123.562902	25.521575
167.078846	6133.970783	25.526592
167.192630	6131.908954	25.531610
166.935075	6137.725015	25.536627
167.058479	6157.433989	25.541645
167.217529	6161.711373	25.546663
167.696414	6186.731585	25.551680
167.676703	6188.306283	25.556698
167.759434	6197.905726	25.561715
167.723273	6223.767389	25.566733
168.262363	6228.030707	25.571751
168.361840	6239.040415	25.576768
168.602164	6243.244506	25.581786
168.602887	6249.886607	25.586803
168.852414	6258.959902	25.591821
169.069575	6276.900230	25.596839
169.238245	6281.589563	25.601856
169.772138	6296.604975	25.606874
170.014405	6301.375857	25.611891
170.252109	6304.135088	25.616909
170.222933	6305.702701	25.621927
170.430336	6326.633780	25.626944
170.953933	6328.877827	25.631962
170.757874	6333.971755	25.636979
170.972409	6327.517898	25.641997
171.265963	6336.206670	25.647015
171.293715	6358.009517	25.652032
171.680985	6347.138335	25.657050
171.753523	6350.822037	25.662067
171.556253	6350.416095	25.667085
172.116499	6362.816976	25.672103
171.881806	6381.488333	25.677120
172.483101	6384.622948	25.682138
172.303927	6391.231093	25.687156
172.607223	6407.163005	25.692173
172.914599	6410.217112	25.697191
172.883027	6427.849078	25.702208
173.215568	6416.369399	25.707226
173.393168	6434.318819	25.712244
173.325424	6442.031715	25.717261
173.641890	6443.431062	25.722279
173.883322	6445.012962	25.727296
174.397020	6448.563003	25.732314
174.266988	6467.435311	25.737332
174.389533	6470.598793	25.742349
174.617929	6466.745749	25.747367
174.505636	6480.421413	25.752384
174.921082	6464.491962	25.757402
174.777466	6491.509996	25.762420
174.851609	6496.591536	25.767437
174.878487	6499.952809	25.772455
174.930933	6518.140433	25.777472
175.485975	6525.052411	25.782490
175.574539	6541.443762	25.787508
175.633076	6565.706346	25.792525
175.914128	6559.551717	25.797543
175.944063	6571.673514	25.802560
176.420759	6585.063511	25.807578
176.512158	6596.522977	25.812596
177.119550	6602.242484	25.817613
177.162860	6603.982437	25.822631
177.075815	6624.358528	25.827648
177.335529	6620.885423	25.832666
177.248964	6633.200624	25.837684
177.297170	6649.523154	25.842701
177.834863	6652.443873	25.847719
177.939664	6678.351467	25.852736
178.170876	6681.398545	25.857754
178.755481	6686.260949	25.862772
178.755228	6694.701614	25.867789
178.893736	6694.409419	25.872807
179.072338	6711.806054	25.877824
179.147106	6707.015870	25.882842
179.425996	6713.711359	25.887860
179.395421	6736.846857	25.892877
179.833210	6732.677890	25.897895
179.887173	6746.657075	25.902912
179.802742	6756.374324	25.907930
180.477932	6770.667356	25.912948
180.393636	6763.598799	25.917965
180.499331	6779.865474	25.922983
180.297314	6805.766570	25.928000
180.733928	6810.715739	25.933018
180.843126	6824.226642	25.938036
180.691312	6841.977431	25.943053
181.372991	6848.675610	25.948071
181.379946	6860.223286	25.953088
181.795474	6867.791794	25.958106
181.993363	6886.581167	25.963124
182.191089	6897.327740	25.968141
182.290928	6913.221380	25.973159
182.506735	6930.052852	25.978176
182.782275	6921.108294	25.983194
183.091250	6950.145798	25.988212
183.427904	6948.407720	25.993229
183.507431	6941.193025	25.998247
183.684374	6955.371794	26.003264
183.793168	6971.090723	26.008282
184.014955	6975.038936	26.013300
184.149688	6983.023401	26.018317
184.786562	6984.611570	26.023335
184.612575	7004.385795	26.028352
184.861014	6995.055786	26.033370
185.173203	6994.359903	26.038388
184.917530	7006.848320	26.043405
185.383522	7011.626491	26.048423
185.511976	7024.663350	26.053440
185.804491	7015.514285	26.058458
186.038013	7028.151733	26.063476
185.942144	7045.947837	26.068493
186.369533	7045.446340	26.073511
186.375511	7056.562677	26.078528
186.687235	7060.721297	26.083546
186.680567	7063.257247	26.088564
186.610428	7090.535094	26.093581
187.078139	7085.062996	26.098599
186.922553	7091.301256	26.103616
187.141158	7103.902637	26.108634
187.259996	7120.670810	26.113652
187.671498	7125.432831	26.118669
187.830123	7147.284410	26.123687
187.628220	7155.463324	26.128704
187.854067	7167.616156	26.133722
188.102522	7175.169147	26.138740
188.273744	7184.950671	26.143757
188.807904	7193.597721	26.148775
188.502880	7211.976073	26.153792
189.037128	7225.593392	26.158810
189.302476	7226.047392	26.163828
189.350110	7240.054841	26.168845
190.063604	7261.739890	26.173863
189.823484	7261.812050	26.178880
190.163556	7265.120060	26.183898
190.727210	7282.020350	26.188916
190.796731	7297.942237	26.193933
190.983338	7292.708800	26.198951
190.745420	7301.559344	26.203968
190.890015	7314.381881	26.208986
191.210046	7326.055296	26.214004
191.315475	7338.271516	26.219021
191.520844	7344.789612	26.224039
191.698299	7364.903099	26.229056
191.804997	7385.719916	26.234074
192.040600	7382.781542	26.239092
191.892058	7407.996564	26.244109
192.580413	7409.751911	26.249127
192.602941	7438.521864	26.254144
192.699818	7443.608609	26.259162
193.404023	7460.577193	26.264180
193.395224	7478.138812	26.269197
193.931345	7483.840510	26.274215
193.863520	7494.535351	26.279232
193.987342	7501.208009	26.284250
194.380913	7509.566580	26.289268
194.427986	7516.454387	26.294285
195.097870	7526.441865	26.299303
195.486360	7527.834904	26.304320
195.512659	7536.862392	26.309338
195.744857	7532.394060	26.314356
195.443169	7541.553830	26.319373
195.994875	7543.422400	26.324391
196.373436	7553.484118	26.329408
196.152117	7573.526825	26.334426
196.566792	7558.528259	26.339444
196.505809	7567.783680	26.344461
196.681239	7572.478579	26.349479
196.872098	7583.133806	26.354496
196.817921	7595.150576	26.359514
197.130796	7609.393285	26.364532
196.955229	7621.338798	26.369549
197.624586	7626.082703	26.374567
197.764118	7641.482126	26.379584
197.764901	7648.034215	26.384602
198.221736	7655.262278	26.389620
198.118445	7675.683364	26.394637
198.309391	7673.773982	26.399655
198.626851	7695.104554	26.404672
198.719637	7709.265632	26.409690
199.387144	7718.416295	26.414708
199.158248	7741.643586	26.419725
199.388855	7734.809979	26.424743
199.935411	7749.602545	26.429760
199.745146	7764.680159	26.434778
200.290417	7763.565198	26.439796
200.202818	7780.299710	26.444813
200.221170	7788.931651	26.449831
200.661351	7804.820253	26.454848
200.780435	7806.562760	26.459866
201.099309	7819.062250	26.464884
201.021239	7830.606588	26.469901
201.269971	7840.960166	26.474919
201.647010	7857.811617	26.479936
202.011759	7863.947497	26.484954
202.308863	7871.167442	26.489972
202.433785	7889.577800	26.494989
202.549019	7893.965311	26.500007
202.977038	7884.920928	26.505024
202.926096	7904.471094	26.510042
203.095273	7916.418835	26.515060
203.199632	7921.339073	26.520077
203.786923	7926.412531	26.525095
203.972543	7944.062210	26.530112
203.537584	7948.161926	26.535130
204.230392	7959.508635	26.540148
204.215958	7980.826003	26.545165
205.106713	7977.671147	26.550183
205.048230	7973.249239	26.555200
204.983604	7992.484327	26.560218
205.523663	7998.335228	26.565236
205.582335	8002.960571	26.570253
205.557060	8013.915752	26.575271
205.744231	8024.115795	26.580288
205.887159	8041.397695	26.585306
206.264845	8049.631571	26.590324
206.220824	8064.753001	26.595341
206.510987	8064.644426	26.600359
206.983161	8085.340999	26.605376
206.913233	8097.301676	26.610394
207.207301	8095.423225	26.615412
207.562730	8114.104471	26.620429
207.411892	8114.078353	26.625447
207.812423	8127.565767	26.630464
207.897477	8145.159846	26.635482
208.129112	8143.801384	26.640500
208.470522	8167.143629	26.645517
208.810279	8175.771412	26.650535
209.035727	8196.546786	26.655552
208.996388	8202.659103	26.660570
209.284705	8198.657873	26.665588
209.553764	8223.516741	26.670605
209.776585	8232.965823	26.675623
210.131379	8244.326944	26.680640
210.188107	8265.933037	26.685658
210.859031	8266.788632	26.690676
210.524251	8268.962380	26.695693
210.972893	8292.164958	26.700711
210.838194	8300.210443	26.705728
210.770101	8311.939382	26.710746
211.605971	8327.896132	26.715764
211.331611	8332.919367	26.720781
211.358496	8353.500948	26.725799
211.828979	8367.852949	26.730816
212.045254	8394.240367	26.735834
212.394587	8390.284131	26.740852
212.516398	8422.029679	26.745869
212.514394	8424.194835	26.750887
212.998292	8447.565106	26.755904
213.292487	8456.354981	26.760922
213.198739	8461.349145	26.765940
213.380666	8472.809943	26.770957
213.635011	8489.039577	26.775975
214.121360	8501.685183	26.780992
214.384915	8516.718312	26.786010
214.383526	8513.485750	26.791028
214.687651	8534.022456	26.796045
215.078634	8543.826729	26.801063
215.261024	8544.066846	26.806080
215.364383	8573.795180	26.811098
215.818440	8569.679770	26.816116
215.872989	8578.006014	26.821133
215.974242	8587.008296	26.826151
216.232983	8600.091047	26.831168
216.248695	8612.408174	26.836186
216.643112	8621.798357	26.841204
217.064037	8635.676701	26.846221
217.250684	8651.474991	26.851239
217.390932	8659.757944	26.856256
217.482405	8667.314790	26.861274
217.858739	8688.799223	26.866292
218.008341	8694.711083	26.871309
218.384290	8702.110567	26.876327
218.674538	8710.196984	26.881344
218.765841	8729.812839	26.886362
218.979612	8729.712969	26.891380
219.087635	8751.422299	26.896397
219.116563	8753.602861	26.901415
219.186581	8761.457137	26.906432
219.675955	8780.387979	26.911450
219.725131	8800.686003	26.916468
219.970688	8827.374939	26.921485
220.200466	8829.494691	26.926503
220.800452	8844.128972	26.931520
220.674723	8856.750143	26.936538
220.806682	8871.217721	26.941556
221.060326	8883.423193	26.946573
221.563143	8911.657026	26.951591
222.118619	8908.583498	26.956608
222.042895	8924.850883	26.961626
222.445238	8940.592483	26.966644
222.653530	8938.435875	26.971661
222.475871	8950.322065	26.976679
222.949006	8967.879591	26.981696
223.107870	8971.884411	26.986714
223.416956	8998.644257	26.991732
223.505892	9006.541999	26.996749
223.474483	9020.089857	27.001767
223.997739	9030.921055	27.006784
224.260830	9038.867973	27.011802
224.289195	9059.922091	27.016820
224.812206	9074.476370	27.021837
224.823954	9090.727868	27.026855
225.149227	9089.777650	27.031872
225.243976	9116.935550	27.036890
225.421695	9115.179443	27.041908
225.684418	9127.514370	27.046925
225.680058	9156.212300	27.051943
226.237236	9167.485434	27.056960
226.483671	9176.434079	27.061978
226.649424	9202.537353	27.066996
226.975622	9199.234669	27.072013
226.909827	9224.376618	27.077031
227.057948	9229.354614	27.082048
227.672720	9248.415719	27.087066
227.801372	9267.105133	27.092084
228.345774	9277.015233	27.097101
228.429986	9289.364080	27.102119
228.940864	9291.702844	27.107136
228.945827	9313.611187	27.112154
229.256461	9312.846934	27.117172
229.419412	9319.598957	27.122189
229.474011	9323.710934	27.127207
229.718448	9335.853678	27.132224
229.960285	9342.847107	27.137242
229.709999	9351.696098	27.142260
230.174347	9367.130859	27.147277
230.367643	9367.775683	27.152295
230.755422	9388.551731	27.157312
230.996498	9396.700994	27.162330
231.166134	9404.169621	27.167348
231.342249	9420.641610	27.172365
231.223127	9437.593410	27.177383
231.516277	9453.118829	27.182400
231.790664	9472.355506	27.187418
232.130255	9499.328569	27.192436
232.825215	9500.901093	27.197453
232.927509	9524.767822	27.202471
233.235384	9521.975446	27.207488
233.225673	9537.889835	27.212506
233.182446	9553.554541	27.217524
233.630189	9566.254652	27.222541
233.575128	9584.858253	27.227559
234.274286	9602.086788	27.232576
234.210732	9614.261821	27.237594
234.354606	9630.469147	27.242612
235.106756	9637.902116	27.247629
234.929140	9667.086563	27.252647
235.123410	9671.207020	27.257664
235.382729	9681.707360	27.262682
235.644409	9695.646864	27.267700
236.105749	9711.997882	27.272717
236.011832	9742.106884	27.277735
236.660715	9747.173889	27.282752
236.600079	9767.843463	27.287770
236.879901	9775.828156	27.292788
237.017713	9802.182038	27.297805
237.310985	9819.931775	27.302823
237.773164	9822.737974	27.307840
237.936289	9859.221352	27.312858
238.177533	9866.653919	27.317876
238.725076	9874.727484	27.322893
238.806033	9885.478071	27.327911
239.111780	9902.191436	27.332928
239.216375	9916.360391	27.337946
239.418066	9932.689228	27.342964
240.196901	9942.148121	27.347981
240.049966	9953.385532	27.352999
239.994940	9952.317811	27.358016
240.582394	9977.118818	27.363034
240.645316	9988.722514	27.368052
241.389095	10003.777599	27.373069
241.319997	10020.840692	27.378087
241.118897	10025.632522	27.383104
241.780991	10046.437280	27.388122
241.706533	10063.327197	27.393140
242.397677	10073.931208	27.398157
242.763763	10086.472718	27.403175
243.007671	10086.211078	27.408192
242.958390	10098.604704	27.413210
242.961254	10115.084025	27.418228
243.558099	10130.458987	27.423245
243.257220	10141.134295	27.428263
243.548138	10150.664627	27.433280
243.899320	10169.364735	27.438298
243.923682	10189.633957	27.443316
244.180542	10200.531321	27.448333
244.382396	10230.338594	27.453351
245.042511	10237.575943	27.458368
245.577319	10263.066792	27.463386
245.336510	10268.526256	27.468404
245.630016	10262.021511	27.473421
245.521700	10290.177737	27.478439
245.665154	10309.907427	27.483456
246.164553	10328.604457	27.488474
246.059080	10346.233278	27.493492
246.512185	10357.722228	27.498509
246.915269	10385.830206	27.503527
247.283251	10390.570483	27.508544
247.725053	10419.349651	27.513562
247.983958	10435.771160	27.518580
248.572263	10436.201741	27.523597
248.521172	10460.905935	27.528615
248.954967	10461.788315	27.533632
249.308002	10477.859453	27.538650
249.250933	10491.204806	27.543668
249.513767	10494.978506	27.548685
249.816511	10510.372578	27.553703
249.783851	10524.056629	27.558720
250.044381	10537.860758	27.563738
250.187049	10556.874730	27.568756
250.823947	10557.856641	27.573773
250.635209	10578.989653	27.578791
250.839770	10592.587223	27.583808
251.456142	10612.072763	27.588826
251.426132	10622.698035	27.593844
252.080461	10636.990131	27.598861
252.070369	10669.271692	27.603879
252.379696	10670.074632	27.608896
252.979928	10693.448622	27.613914
253.018930	10722.162649	27.618932
253.529723	10717.409393	27.623949
253.881325	10738.538257	27.628967
254.131358	10745.129137	27.633984
254.273646	10747.499198	27.639002
253.939379	10773.804395	27.644020
254.544852	10782.865469	27.649037
254.763660	10802.317781	27.654055
255.068064	10811.225442	27.659072
255.478033	10821.918252	27.664090
255.102651	10844.960760	27.669108
255.758776	10858.947067	27.674125
256.218016	10874.897812	27.679143
256.198424	10898.926205	27.684160
256.417642	10908.987269	27.689178
256.292443	10929.060787	27.694196
257.200049	10947.375033	27.699213
256.962245	10969.947437	27.704231
257.622964	10984.799746	27.709248
257.762693	11000.303998	27.714266
257.653759	11018.859079	27.719284
258.252882	11039.477796	27.724301
258.775539	11069.568360	27.729319
258.755733	11082.915124	27.734336
259.075917	11090.892216	27.739354
259.179228	11100.966284	27.744372
259.863957	11117.574846	27.749389
260.012191	11134.549564	27.754407
260.391339	11151.126806	27.759424
260.799139	11170.868154	27.764442
260.678351	11171.652501	27.769460
261.032077	11188.150474	27.774477
261.385214	11202.511841	27.779495
261.411564	11219.295673	27.784512
261.751980	11225.816637	27.789530
261.584291	11249.969338	27.794548
261.919705	11252.266537	27.799565
262.120834	11276.668650	27.804583
262.306990	11294.409381	27.809600
262.646833	11303.076660	27.814618
262.847609	11330.728137	27.819636
263.475581	11355.516686	27.824653
263.724856	11366.469672	27.829671
263.861772	11379.543342	27.834688
264.371894	11390.054496	27.839706
264.339299	11415.121089	27.844724
264.652457	11427.859924	27.849741
264.943968	11440.060286	27.854759
265.202888	11461.126649	27.859776
265.570340	11477.419371	27.864794
265.561854	11500.091646	27.869812
266.040408	11516.969542	27.874829
266.831045	11526.124876	27.879847
266.510071	11557.134433	27.884864
267.007173	11567.127849	27.889882
267.081373	11586.543586	27.894900
267.067589	11595.071009	27.899917
268.059985	11610.701012	27.904935
268.090790	11623.130611	27.909952
268.220740	11638.949101	27.914970
268.604588	11664.864258	27.919988
268.823437	11675.991101	27.925005
268.729893	11693.550078	27.930023
268.845449	11716.024057	27.935040
269.556838	11731.062493	27.940058
269.495958	11752.725825	27.945076
269.900051	11773.015328	27.950093
270.187849	11788.303576	27.955111
270.217321	11821.895111	27.960128
270.790168	11843.475725	27.965146
270.849127	11860.623563	27.970164
271.343583	11880.230097	27.975181
271.821001	11904.596878	27.980199
271.979943	11917.328535	27.985216
272.532916	11926.918971	27.990234
272.851486	11948.708853	27.995252
272.922622	11969.422460	28.000269
273.496124	11981.409515	28.005287
273.866591	12000.660096	28.010304
273.776313	12007.684449	28.015322
274.248624	12023.210268	28.020340
274.555216	12033.164597	28.025357
274.580038	12051.950852	28.030375
274.723027	12068.758803	28.035392
275.006760	12086.391276	28.040410
275.212067	12099.066550	28.045428
275.635363	12114.368922	28.050445
275.768263	12134.341325	28.055463
275.966224	12154.638639	28.060480
276.675623	12170.825031	28.065498
276.593046	12199.676837	28.070516
276.708248	12207.863333	28.075533
277.379113	12221.821599	28.080551
277.762720	12246.540080	28.085568
277.897192	12258.871061	28.090586
277.930597	12282.040192	28.095604
278.365921	12293.486195	28.100621
278.519258	12315.359076	28.105639
278.822777	12341.148360	28.110656
279.271700	12358.315695	28.115674
279.331884	12375.208584	28.120692
279.529474	12389.374556	28.125709
280.082873	12414.470186	28.130727
280.108791	12435.264362	28.135744
280.557187	12454.512038	28.140762
280.677993	12471.918183	28.145780
280.811270	12484.946071	28.150797
281.451605	12502.275707	28.155815
281.358700	12522.207170	28.160832
281.882616	12534.393527	28.165850
281.953877	12559.391113	28.170868
282.180754	12581.832105	28.175885
282.515014	12599.978391	28.180903
282.873163	12630.905945	28.185920
283.362632	12636.268168	28.190938
283.277497	12656.390768	28.195956
283.608940	12674.501358	28.200973
284.219172	12691.995347	28.205991
284.419747	12714.888431	28.211008
285.043177	12718.291727	28.216026
285.132714	12753.408594	28.221044
285.407055	12768.389542	28.226061
285.671912	12783.383105	28.231079
285.533789	12799.875885	28.236096
286.356875	12819.195926	28.241114
286.409834	12833.958281	28.246132
286.289444	12858.997505	28.251149
286.626601	12877.554936	28.256167
286.863745	12903.433319	28.261184
286.988968	12932.501021	28.266202
287.422097	12959.434438	28.271220
287.915335	12997.553330	28.276237
288.091984	13020.652523	28.281255
288.414181	13040.186539	28.286272
289.129235	13059.852542	28.291290
289.050926	13088.451489	28.296308
289.182545	13104.800644	28.301325
289.788979	13127.122828	28.306343
290.701999	13148.366781	28.311360
290.472769	13164.101222	28.316378
290.509110	13203.088922	28.321396
290.785181	13215.302633	28.326413
291.845888	13220.660328	28.331431
291.899168	13248.341059	28.336448
291.932169	13269.576392	28.341466
291.940644	13299.097459	28.346484
292.737425	13319.714735	28.351501
293.837705	13306.929795	28.356519
293.455315	13345.567942	28.361536
292.781546	13368.940773	28.366554
293.934989	13380.103203	28.371572
294.465887	13389.111906	28.376589
294.523233	13416.377770	28.381607
294.321822	13446.430274	28.386624
295.197356	13461.173663	28.391642
296.337754	13467.238470	28.396660
296.073850	13486.520170	28.401677
295.657587	13514.890551	28.406695
296.011273	13527.737800	28.411712
297.236074	13521.754495	28.416730
297.179711	13552.834362	28.421748
296.555743	13584.805688	28.426765
296.872099	13600.930916	28.431783
298.017010	13618.682544	28.436800
297.997155	13626.195522	28.441818
297.700478	13663.858879	28.446836
297.709865	13698.061209	28.451853
298.809371	13701.018711	28.456871
298.960948	13733.566425	28.461888
299.163433	13755.510327	28.466906
299.399400	13777.617349	28.471924
300.014058	13805.724607	28.476941
300.370893	13809.348781	28.481959
300.233218	13834.718592	28.486976
300.396847	13855.069412	28.491994
300.800395	13880.931258	28.497012
300.599442	13905.812057	28.502029
301.564933	13925.823781	28.507047
301.580911	13960.250938	28.512064
301.987177	13976.095307	28.517082
302.711385	14000.172219	28.522100
302.733247	14029.832654	28.527117
303.037197	14052.808218	28.532135
303.282770	14073.133137	28.537152
303.941372	14092.278613	28.542170
304.333805	14110.743193	28.547188
304.186637	14133.100084	28.552205
304.700565	14148.249105	28.557223
304.973004	14168.397908	28.562240
305.544087	14194.593433	28.567258
305.769076	14216.436513	28.572276
305.883883	14242.644597	28.577293
306.439511	14252.056308	28.582311
306.541470	14275.872555	28.587328
306.995793	14298.856671	28.592346
307.449676	14308.308896	28.597364
307.419465	14334.383525	28.602381
307.826187	14345.250995	28.607399
307.947729	14379.284881	28.612416
308.014314	14397.029873	28.617434
308.740279	14422.153622	28.622452
308.633393	14447.133148	28.627469
309.098446	14480.513057	28.632487
309.462921	14504.022980	28.637504
309.882958	14530.783062	28.642522
310.275306	14554.026815	28.647540
310.306829	14585.166591	28.652557
310.754343	14603.805436	28.657575
311.375152	14629.361419	28.662592
311.599832	14654.877411	28.667610
311.785735	14665.272568	28.672628
311.995234	14696.239672	28.677645
312.686403	14721.461054	28.682663
312.932428	14746.390501	28.687680
313.194380	14763.621268	28.692698
313.781053	14787.622813	28.697716
313.719690	14805.370511	28.702733
314.205905	14826.495020	28.707751
314.391888	14841.082709	28.712768
314.683451	14868.658964	28.717786
315.372603	14881.795345	28.722804
315.519369	14906.661084	28.727821
315.846347	14919.992988	28.732839
315.985077	14951.290661	28.737856
316.371835	14967.389823	28.742874
316.549425	14982.251696	28.747892
316.337139	15018.213012	28.752909
317.322721	15040.796589	28.757927
317.485108	15067.844492	28.762944
317.508476	15102.250754	28.767962
318.259415	15110.823657	28.772980
318.159339	15146.697330	28.777997
318.690233	15166.364840	28.783015
319.216319	15186.138769	28.788032
319.239996	15208.907010	28.793050
319.754526	15239.971231	28.798068
320.012630	15266.719913	28.803085
320.683675	15285.465965	28.808103
320.595302	15305.042274	28.813120
321.052893	15337.815193	28.818138
321.509343	15358.278602	28.823156
321.628202	15373.738454	28.828173
322.145436	15389.865296	28.833191
322.475798	15412.770620	28.838208
322.405563	15426.725066	28.843226
322.821387	15442.208333	28.848244
322.975285	15470.958983	28.853261
323.449668	15505.266216	28.858279
323.559911	15521.496804	28.863296
323.577781	15554.981285	28.868314
324.121517	15584.258672	28.873332
324.535115	15609.185334	28.878349
324.651900	15631.301971	28.883367
325.204350	15665.413780	28.888384
325.132973	15694.180038	28.893402
325.736016	15715.625235	28.898420
325.954303	15754.049821	28.903437
326.551204	15777.305583	28.908455
327.013016	15806.102000	28.913472
327.034472	15836.229160	28.918490
327.470003	15859.530662	28.923508
327.826816	15895.352407	28.928525
328.346660	15911.386333	28.933543
328.615048	15939.967534	28.938560
328.999352	15970.523507	28.943578
329.102718	15989.041201	28.948596
329.304962	16025.930690	28.953613
329.450190	16058.094732	28.958631
330.102901	16085.211313	28.963648
330.100639	16110.745057	28.968666
330.697963	16149.818705	28.973684
331.007960	16187.489868	28.978701
331.386718	16217.999930	28.983719
331.938341	16244.304405	28.988736
331.957919	16279.990501	28.993754
332.479124	16303.875846	28.998772
332.807403	16344.651119	29.003789
333.275442	16366.754738	29.008807
333.601527	16394.580033	29.013824
333.902180	16421.843709	29.018842
334.500635	16448.694025	29.023860
334.913180	16474.140758	29.028877
335.070367	16494.098691	29.033895
335.528132	16512.629245	29.038912
335.749872	16540.897648	29.043930
336.270243	16558.885114	29.048948
336.696478	16593.119037	29.053965
336.877714	16613.342677	29.058983
337.473537	16635.261573	29.064000
337.684035	16669.078971	29.069018
338.269619	16694.707049	29.074036
338.135315	16709.819136	29.079053
338.326914	16730.941262	29.084071
338.789991	16770.640739	29.089088
338.907928	16791.347959	29.094106
339.483347	16813.394996	29.099124
339.804479	16846.510334	29.104141
339.984299	16882.929404	29.109159
340.558991	16900.337630	29.114176
340.693748	16925.723848	29.119194
341.051053	16944.728642	29.124212
341.487470	16975.046130	29.129229
341.619612	17005.511766	29.134247
342.106097	17035.133806	29.139264
342.294058	17060.498813	29.144282
342.761960	17084.926906	29.149300
342.817811	17120.076010	29.154317
343.068243	17155.158304	29.159335
344.087924	17171.646680	29.164352
344.246940	17191.718647	29.169370
344.555596	17207.047916	29.174388
344.773758	17240.758020	29.179405
345.183729	17266.316741	29.184423
345.625140	17289.083334	29.189440
345.588879	17324.479838	29.194458
346.299156	17334.534523	29.199476
346.551616	17373.095929	29.204493
346.712488	17391.637199	29.209511
347.152853	17416.633094	29.214528
347.414419	17456.559882	29.219546
348.045913	17469.017440	29.224564
348.134620	17497.957376	29.229581
348.211629	17522.915837	29.234599
349.189576	17557.683102	29.239616
349.211354	17596.745081	29.244634
349.436765	17612.460526	29.249652
349.694933	17637.433313	29.254669
350.062002	17671.040826	29.259687
350.693090	17700.725247	29.264704
350.832862	17735.124017	29.269722
350.857367	17774.684098	29.274740
351.685523	17807.255555	29.279757
351.762912	17835.472812	29.284775
352.453201	17874.098484	29.289792
352.341988	17911.182770	29.294810
353.047320	17940.426551	29.299828
353.110522	17968.275928	29.304845
353.443295	18001.511448	29.309863
354.049686	18026.504430	29.314880
354.406005	18062.849580	29.319898
354.919533	18099.116769	29.324916
355.212443	18128.280958	29.329933
355.473650	18163.505473	29.334951
356.419080	18196.058283	29.339968
356.324898	18225.050245	29.344986
356.587893	18242.886663	29.350004
357.202684	18268.895415	29.355021
357.467355	18305.262569	29.360039
358.155969	18329.067954	29.365056
358.101663	18359.084538	29.370074
358.778025	18392.200914	29.375092
359.321276	18422.238520	29.380109
359.362145	18443.710940	29.385127
359.933682	18477.656706	29.390144
359.832337	18505.050242	29.395162
360.213796	18535.404898	29.400180
360.408051	18564.994481	29.405197
360.890200	18593.294216	29.410215
361.444693	18635.675615	29.415232
362.038319	18666.329604	29.420250
362.446049	18691.042747	29.425268
362.580467	18723.834867	29.430285
362.776521	18751.341961	29.435303
363.337305	18766.485905	29.440320
363.692040	18803.827690	29.445338
364.160824	18828.132082	29.450356
364.526941	18859.722676	29.455373
364.752760	18877.567503	29.460391
365.067835	18905.575394	29.465408
365.446113	18943.961962	29.470426
365.701316	18972.988830	29.475444
365.966624	19002.187492	29.480461
366.042548	19045.405856	29.485479
366.694528	19078.806673	29.490496
367.082617	19108.079789	29.495514
367.434758	19146.491642	29.500532
367.891830	19178.184446	29.505549
368.226994	19215.508319	29.510567
368.331816	19240.800543	29.515584
368.817005	19265.648334	29.520602
369.269487	19290.736477	29.525620
369.625922	19317.700858	29.530637
369.688316	19356.205290	29.535655
370.248378	19380.938385	29.540672
370.744293	19411.890539	29.545690
370.905424	19451.146621	29.550708
371.402438	19467.347003	29.555725
371.969239	19516.356386	29.560743
372.517293	19538.706387	29.565760
372.785091	19563.992621	29.570778
372.893297	19596.611060	29.575796
373.510188	19626.238201	29.580813
373.455320	19667.956861	29.585831
373.957321	19694.650238	29.590848
374.434898	19736.804366	29.595866
374.829041	19762.041610	29.600884
375.294112	19789.947327	29.605901
375.436275	19834.646623	29.610919
375.795712	19867.939776	29.615936
376.378250	19896.641322	29.620954
376.673264	19928.745478	29.625972
376.791680	19960.904149	29.630989
377.256714	19995.578513	29.636007
378.261514	20026.163793	29.641024
378.552332	20075.165304	29.646042
378.977074	20099.067341	29.651060
379.111001	20129.596714	29.656077
379.645282	20159.284191	29.661095
380.161278	20188.746138	29.666112
380.000281	20222.545506	29.671130
380.279912	20260.409060	29.676148
381.205214	20289.043513	29.681165
381.353656	20324.877741	29.686183
381.789461	20351.504288	29.691200
382.273431	20400.928850	29.696218
382.666687	20430.892408	29.701236
383.072181	20457.478417	29.706253
383.286110	20493.059364	29.711271
383.899388	20528.700423	29.716288
384.170664	20558.482587	29.721306
384.427631	20597.017570	29.726324
385.206689	20616.611058	29.731341
385.695099	20655.973453	29.736359
385.997829	20669.548917	29.741376
386.215012	20701.803022	29.746394
386.459667	20740.799179	29.751412
386.881980	20765.700594	29.756429
387.057665	20802.248711	29.761447
387.646547	20841.832989	29.766464
388.119109	20877.283649	29.771482
388.654704	20911.252911	29.776500
388.385252	20942.714536	29.781517
388.989932	20991.573745	29.786535
389.565081	21014.304364	29.791552
389.800673	21044.692434	29.796570
390.088053	21082.335815	29.801588
390.597256	21117.512878	29.806605
390.903583	21158.059146	29.811623
391.566607	21187.014463	29.816640
391.800200	21222.032386	29.821658
392.314708	21258.599521	29.826676
392.621883	21287.807839	29.831693
392.790909	21339.723299	29.836711
393.560032	21367.568701	29.841728
393.896201	21390.366183	29.846746
393.741624	21434.693117	29.851764
394.718331	21460.908670	29.856781
394.644624	21498.918625	29.861799
394.862585	21526.499165	29.866816
395.505412	21556.390310	29.871834
395.887741	21596.095686	29.876852
396.729432	21629.908519	29.881869
396.613000	21660.816366	29.886887
396.922074	21697.058951	29.891904
397.568849	21730.238854	29.896922
398.048413	21765.821092	29.901940
398.653971	21794.569370	29.906957
398.952337	21830.120238	29.911975
399.399954	21862.392033	29.916992
399.698812	21901.829700	29.922010
399.978599	21938.873919	29.927028
400.381534	21968.926907	29.932045
400.606785	22017.881838	29.937063
401.092817	22050.543406	29.942080
401.757312	22084.679757	29.947098
401.948769	22124.178290	29.952116
402.467343	22158.785172	29.957133
402.687958	22200.880767	29.962151
403.078056	22235.867002	29.967168
403.526532	22270.365876	29.972186
403.848336	22306.500436	29.977204
404.430401	22336.872906	29.982221
404.867201	22376.936918	29.987239
405.343948	22416.981800	29.992256
405.593009	22462.121325	29.997274
405.771760	22498.529106	30.002292
406.746917	22532.791552	30.007309
407.114878	22579.302474	30.012327
407.422026	22614.345792	30.017344
407.547479	22643.066166	30.022362
408.342384	22691.824693	30.027380
408.660641	22722.172132	30.032397
408.990446	22769.028911	30.037415
409.593692	22807.090598	30.042432
409.690001	22835.909155	30.047450
410.206230	22876.822165	30.052468
410.699455	22912.041871	30.057485
411.033915	22956.641903	30.062503
411.160955	22987.753129	30.067520
412.072698	23026.827065	30.072538
412.244884	23068.723100	30.077556
412.524404	23108.122616	30.082573
412.916053	23149.738113	30.087591
413.544502	23187.634062	30.092608
413.904108	23221.924082	30.097626
414.356097	23263.282299	30.102644
415.029082	23299.646268	30.107661
415.318930	23349.589366	30.112679
415.607231	23384.635812	30.117696
416.199289	23415.580977	30.122714
416.174783	23457.264519	30.127732
416.791479	23491.755380	30.132749
416.958884	23534.837616	30.137767
417.324379	23574.905212	30.142784
418.195284	23620.985668	30.147802
418.378861	23661.760078	30.152820
419.016509	23692.777048	30.157837
419.172163	23736.106161	30.162855
419.339888	23782.538390	30.167872
419.764274	23824.711509	30.172890
420.182297	23864.233352	30.177908
420.819243	23905.586171	30.182925
421.387503	23946.912611	30.187943
421.692267	23997.425994	30.192960
422.191106	24026.589956	30.197978
422.295950	24064.044646	30.202996
423.007164	24100.654737	30.208013
423.264119	24136.434899	30.213031
423.688463	24169.427718	30.218048
424.168768	24213.749852	30.223066
424.523741	24255.736822	30.228084
425.045420	24297.409293	30.233101
425.456567	24331.404422	30.238119
425.770134	24373.862170	30.243136
426.528671	24414.795543	30.248154
426.523724	24460.535919	30.253172
426.848055	24497.384357	30.258189
427.240122	24546.724232	30.263207
427.587482	24597.222872	30.268224
428.285618	24628.458624	30.273242
428.647000	24673.681607	30.278260
429.019135	24723.211378	30.283277
429.729753	24769.553284	30.288295
430.195250	24809.835893	30.293312
430.879137	24853.416324	30.298330
431.284787	24900.553418	30.303348
431.693510	24931.541133	30.308365
431.987914	24963.295346	30.313383
432.209330	25009.195276	30.318400
432.818076	25052.952663	30.323418
433.401132	25106.258814	30.328436
433.368259	25141.779932	30.333453
434.242994	25188.900117	30.338471
434.458094	25234.795387	30.343488
435.242202	25269.941851	30.348506
435.377013	25311.507332	30.353524
435.913062	25357.968034	30.358541
436.341740	25393.867491	30.363559
436.971426	25449.195131	30.368576
437.678326	25488.291255	30.373594
437.707728	25536.120043	30.378612
438.035419	25569.831787	30.383629
438.564690	25615.877951	30.388647
438.732864	25666.138122	30.393664
439.374737	25701.419406	30.398682
439.873462	25759.264720	30.403700
440.119090	25800.115951	30.408717
440.923448	25846.779603	30.413735
441.360018	25899.484754	30.418752
441.741064	25919.912006	30.423770
441.608649	25963.179279	30.428788
442.322485	26016.709488	30.433805
443.108678	26064.884492	30.438823
443.367531	26119.398755	30.443840
444.021642	26158.520911	30.448858
444.028859	26202.601571	30.453876
444.579801	26247.462961	30.458893
445.562221	26293.599971	30.463911
445.548272	26341.964941	30.468928
445.968036	26380.552288	30.473946
446.341211	26437.673068	30.478964
446.891737	26479.185183	30.483981
447.543021	26514.151137	30.488999
447.775311	26557.984112	30.494016
448.424231	26601.965904	30.499034
448.777209	26659.996075	30.504052
449.064324	26698.054060	30.509069
449.428363	26746.354453	30.514087
450.032147	26790.706955	30.519104
450.568455	26839.089504	30.524122
450.878736	26881.654921	30.529140
451.362073	26921.034186	30.534157
451.836966	26963.149864	30.539175
452.148413	27004.592399	30.544192
452.792247	27035.548145	30.549210
453.565199	27083.264473	30.554228
453.617791	27114.810304	30.559245
453.964070	27155.701707	30.564263
454.263941	27207.345163	30.569280
454.764294	27244.911657	30.574298
455.312606	27292.539555	30.579316
455.766706	27342.861379	30.584333
456.458005	27373.945522	30.589351
456.353463	27435.650183	30.594368
457.097900	27474.060058	30.599386
457.609418	27530.177322	30.604404
458.232236	27564.743171	30.609421
458.663672	27614.763539	30.614439
458.869567	27666.039050	30.619456
459.565483	27711.388135	30.624474
459.728954	27758.273417	30.629492
460.114639	27808.629994	30.634509
460.835688	27855.672484	30.639527
460.897630	27909.467849	30.644544
461.626884	27950.950759	30.649562
462.295309	28003.157056	30.654580
462.794177	28063.776681	30.659597
463.378893	28102.283780	30.664615
463.706611	28158.077007	30.669632
464.188931	28194.266786	30.674650
465.038915	28243.696022	30.679668
465.194085	28295.981822	30.684685
465.886271	28342.554045	30.689703
465.987908	28386.517359	30.694720
466.574080	28421.718769	30.699738
467.040028	28465.480032	30.704756
467.314023	28520.914206	30.709773
468.116582	28566.364598	30.714791
468.432870	28612.980819	30.719808
468.763257	28661.074422	30.724826
469.448315	28709.207265	30.729844
469.877778	28766.897403	30.734861
470.189178	28807.031843	30.739879
471.030502	28866.436620	30.744896
471.381945	28909.627995	30.749914
471.914170	28952.811645	30.754932
471.883077	29004.477339	30.759949
472.659637	29050.545334	30.764967
473.140171	29101.303234	30.769984
473.516580	29155.864352	30.775002
474.027069	29201.008230	30.780020
474.621199	29257.738895	30.785037
475.327362	29295.335700	30.790055
475.597673	29347.911617	30.795072
476.509658	29397.087781	30.800090
476.673983	29438.875942	30.805108
476.693933	29495.617211	30.810125
477.489504	29546.617678	30.815143
477.767246	29596.246398	30.820160
478.532084	29642.071807	30.825178
479.144884	29695.775201	30.830196
479.345666	29747.975762	30.835213
480.272698	29782.372627	30.840231
480.714803	29838.524574	30.845248
480.793163	29883.593435	30.850266
481.534458	29917.355596	30.855284
482.075224	29978.798384	30.860301
482.478048	30023.239699	30.865319
482.808384	30055.804967	30.870336
483.293703	30099.201128	30.875354
483.845694	30137.096587	30.880372
484.150695	30185.372103	30.885389
484.543072	30228.241294	30.890407
484.782429	30274.076434	30.895424
485.312988	30325.924409	30.900442
485.543658	30377.415156	30.905460
486.250785	30426.404097	30.910477
487.035246	30476.263807	30.915495
487.371057	30527.062401	30.920512
487.827477	30574.335843	30.925530
488.551246	30626.717500	30.930548
489.141128	30670.962276	30.935565
489.741846	30714.444980	30.940583
490.455489	30765.408910	30.945600
490.606701	30807.284527	30.950618
491.330186	30846.538255	30.955636
491.447787	30894.297725	30.960653
492.066733	30947.073147	30.965671
492.345286	30993.597815	30.970688
493.010202	31038.064582	30.975706
493.511301	31081.242845	30.980724
493.913333	31134.117826	30.985741
494.457786	31187.165023	30.990759
494.806391	31238.891188	30.995776
495.110030	31294.856136	31.000794
495.682647	31345.330774	31.005812
496.172597	31404.455207	31.010829
496.796819	31451.662215	31.015847
497.175291	31515.330136	31.020864
497.615067	31566.780285	31.025882
498.037516	31619.568147	31.030900
498.505601	31677.169941	31.035917
499.200001	31738.344170	31.040935
499.776856	31803.346558	31.045952
499.942136	31850.599020	31.050970
501.098148	31913.786313	31.055988
501.064953	31963.208097	31.061005
501.570289	32014.061799	31.066023
502.428036	32070.887279	31.071040
502.831755	32117.889587	31.076058
503.276995	32176.102620	31.081076
503.564973	32234.098899	31.086093
504.132613	32289.127165	31.091111
504.818558	32349.093218	31.096128
505.519853	32403.538054	31.101146
506.173494	32450.477800	31.106164
506.564539	32514.301846	31.111181
507.110232	32554.996129	31.116199
507.403313	32619.647720	31.121216
507.709588	32678.368183	31.126234
508.597174	32721.985064	31.131252
509.023901	32778.720048	31.136269
509.551859	32824.892702	31.141287
510.096400	32889.074511	31.146304
510.788148	32936.615100	31.151322
511.248067	32989.236747	31.156340
511.395782	33045.390794	31.161357
512.185004	33104.364083	31.166375
512.768462	33157.041518	31.171392
513.197039	33218.021853	31.176410
514.018246	33264.330148	31.181428
514.556217	33320.439420	31.186445
514.637806	33363.525411	31.191463
515.125978	33411.858303	31.196480
515.360957	33480.060087	31.201498
516.193519	33519.885488	31.206516
516.567733	33574.583681	31.211533
517.274785	33620.387953	31.216551
517.602011	33668.164373	31.221568
518.238510	33729.651672	31.226586
518.978826	33767.081948	31.231604
519.170509	33816.222360	31.236621
519.890399	33866.875448	31.241639
520.499401	33917.158876	31.246656
520.540165	33965.232792	31.251674
521.339999	34011.552877	31.256692
521.773973	34063.595020	31.261709
522.253275	34112.780171	31.266727
522.917299	34175.249043	31.271744
523.084928	34231.605491	31.276762
523.867095	34278.033331	31.281780
524.286309	34338.709774	31.286797
524.704982	34388.546341	31.291815
525.313697	34444.085702	31.296832
526.038832	34513.355878	31.301850
526.742800	34567.412405	31.306868
526.851164	34620.428390	31.311885
527.656194	34667.711846	31.316903
528.086171	34722.801958	31.321920
528.547582	34782.510384	31.326938
529.139278	34841.013996	31.331956
529.809276	34896.074392	31.336973
530.208180	34945.051063	31.341991
530.552838	35006.720429	31.347008
531.255527	35075.207511	31.352026
531.548922	35122.204426	31.357044
532.004444	35194.687238	31.362061
532.381355	35249.194428	31.367079
533.374066	35316.681344	31.372096
533.849475	35372.460242	31.377114
534.581587	35434.256321	31.382132
534.852459	35497.975188	31.387149
535.179009	35559.936641	31.392167
535.637334	35619.720944	31.397184
536.509107	35694.885783	31.402202
537.004825	35748.828834	31.407220
537.639579	35819.154177	31.412237
538.098508	35874.839519	31.417255
538.809754	35929.776323	31.422272
539.244280	35999.431697	31.427290
539.700330	36051.498036	31.432308
540.260038	36115.234411	31.437325
541.035821	36181.851507	31.442343
541.449776	36238.107199	31.447360
542.110781	36312.946534	31.452378
542.925376	36368.227372	31.457396
543.268277	36421.579114	31.462413
543.516907	36477.001274	31.467431
544.471091	36533.304212	31.472448
544.666764	36606.492173	31.477466
545.434642	36660.512849	31.482484
545.628848	36721.543855	31.487501
546.308781	36784.031774	31.492519
547.285412	36848.374022	31.497536
547.532768	36916.602562	31.502554
548.155186	36972.930200	31.507572
548.703405	37037.025224	31.512589
548.874365	37097.332243	31.517607
549.647682	37157.366200	31.522624
550.379062	37219.427322	31.527642
550.856164	37278.636400	31.532660
551.368717	37344.853135	31.537677
551.654381	37393.078726	31.542695
552.723787	37450.650075	31.547712
553.002769	37513.159503	31.552730
553.750644	37569.588177	31.557748
554.130077	37617.483212	31.562765
554.544876	37672.035621	31.567783
554.972794	37727.327772	31.572800
555.325679	37797.713748	31.577818
556.162805	37851.240428	31.582836
556.886182	37900.708004	31.587853
557.043741	37961.042198	31.592871
557.712701	38018.659511	31.597888
558.005175	38090.622203	31.602906
558.693259	38150.910278	31.607924
559.118815	38229.773605	31.612941
559.298254	38289.878000	31.617959
560.106577	38354.480699	31.622976
560.395967	38439.434235	31.627994
560.968334	38502.324638	31.633012
561.590375	38580.080595	31.638029
561.896723	38659.640998	31.643047
562.826571	38729.818312	31.648064
563.500691	38809.858288	31.653082
563.890519	38881.833239	31.658100
564.555705	38956.559654	31.663117
565.407309	39024.342564	31.668135
566.032598	39086.020396	31.673152
566.570578	39174.357982	31.678170
567.412883	39234.832455	31.683188
567.967582	39296.885690	31.688205
568.587975	39366.318015	31.693223
569.193282	39424.890980	31.698240
569.585987	39500.520156	31.703258
570.269696	39562.881241	31.708276
571.114275	39636.561135	31.713293
571.547091	39708.955219	31.718311
572.161750	39767.120512	31.723328
572.904096	39834.785601	31.728346
573.207372	39894.265514	31.733364
573.967007	39968.664751	31.738381
574.532713	40029.260214	31.743399
575.005156	40081.101753	31.748416
575.527618	40153.526949	31.753434
576.082701	40211.848720	31.758452
576.904034	40279.246674	31.763469
577.364876	40354.590288	31.768487
578.163302	40412.436789	31.773504
578.568586	40479.591786	31.778522
579.360553	40539.242318	31.783540
579.810570	40605.108684	31.788557
580.055180	40677.427224	31.793575
580.642902	40730.110190	31.798592
581.458484	40807.218489	31.803610
581.812832	40875.807122	31.808628
582.666228	40948.212255	31.813645
583.209768	41021.824380	31.818663
583.933025	41073.264162	31.823680
584.532259	41146.725507	31.828698
585.053930	41201.381223	31.833716
585.952024	41263.785208	31.838733
586.161619	41327.480879	31.843751
587.027337	41390.042183	31.848768
587.230827	41457.076269	31.853786
588.034525	41521.397269	31.858804
588.723048	41581.065124	31.863821
589.350528	41658.908961	31.868839
589.711436	41709.277081	31.873856
590.476410	41787.698552	31.878874
590.696216	41847.280647	31.883892
590.960080	41906.438906	31.888909
591.771734	41969.762503	31.893927
592.459633	42018.094695	31.898944
592.967729	42088.566121	31.903962
593.867290	42156.968262	31.908980
594.001129	42217.348737	31.913997
594.665067	42283.779224	31.919015
595.141072	42350.140013	31.924032
595.734289	42413.766467	31.929050
596.816935	42477.309005	31.934068
597.419582	42541.682592	31.939085
597.583923	42607.000311	31.944103
598.288793	42668.658004	31.949120
598.693117	42744.064885	31.954138
598.883464	42812.179492	31.959156
599.535324	42883.037425	31.964173
600.132984	42971.127539	31.969191
600.889901	43042.495962	31.974208
601.445126	43112.890849	31.979226
602.222216	43185.831977	31.984244
602.833380	43265.465960	31.989261
603.393510	43330.518658	31.994279
604.103559	43414.260399	31.999296
604.657135	43487.972193	32.004314
604.881211	43564.457294	32.009332
605.289497	43637.565396	32.014349
606.343710	43729.744991	32.019367
607.407312	43804.993400	32.024384
607.760402	43882.298327	32.029402
608.666304	43951.135413	32.034420
609.434565	44028.078610	32.039437
609.542074	44102.962262	32.044455
610.731983	44161.743960	32.049472
611.255083	44252.735221	32.054490
612.014022	44318.566778	32.059508
612.830748	44382.687103	32.064525
613.052530	44462.668459	32.069543
613.675753	44525.697207	32.074560
614.193313	44595.526067	32.079578
614.973136	44669.539774	32.084596
615.361853	44737.334903	32.089613
615.757702	44824.216717	32.094631
616.606185	44894.601352	32.099648
617.093678	44970.998078	32.104666
617.801061	45044.172687	32.109684
618.874080	45118.379631	32.114701
619.045952	45198.384997	32.119719
619.739081	45271.430226	32.124736
620.235694	45345.853421	32.129754
620.688860	45419.927278	32.134772
621.364389	45488.637595	32.139789
622.359626	45582.579088	32.144807
623.251846	45650.856273	32.149824
623.519898	45729.338580	32.154842
624.247567	45807.151515	32.159860
625.300909	45861.363435	32.164877
625.480554	45944.632643	32.169895
626.358265	46012.218823	32.174912
626.945567	46084.994190	32.179930
627.807721	46164.974703	32.184948
628.186907	46224.241178	32.189965
628.937397	46299.324001	32.194983
629.361271	46366.023389	32.200000
630.084788	46437.539698	32.205018
630.302289	46506.787380	32.210036
631.557577	46577.537297	32.215053
631.568338	46657.717587	32.220071
632.217385	46732.572593	32.225088
633.270281	46802.090512	32.230106
633.624844	46870.388414	32.235124
634.455173	46928.780336	32.240141
634.639606	46998.101595	32.245159
635.530517	47067.669391	32.250176
635.922339	47132.920952	32.255194
636.602781	47197.487075	32.260212
637.609054	47273.740943	32.265229
638.132690	47337.528194	32.270247
638.540177	47407.354058	32.275264
639.247461	47481.788677	32.280282
639.647266	47552.866926	32.285300
640.151198	47631.810721	32.290317
640.800768	47716.162629	32.295335
641.329472	47790.675368	32.300352
642.112683	47864.723107	32.305370
642.553547	47951.463364	32.310388
643.189341	48025.687705	32.315405
643.920688	48104.946383	32.320423
644.566629	48195.301464	32.325440
645.065987	48272.887501	32.330458
645.811009	48352.546030	32.335476
646.584829	48431.745346	32.340493
647.136026	48525.610617	32.345511
647.988522	48608.246407	32.350528
648.797562	48683.982691	32.355546
648.904804	48774.518055	32.360564
649.995546	48850.821093	32.365581
650.694625	48939.528598	32.370599
651.289723	49013.428722	32.375616
651.952097	49093.963057	32.380634
652.410400	49188.383846	32.385652
653.393426	49261.803850	32.390669
653.879961	49350.071505	32.395687
654.329618	49437.455009	32.400704
655.180279	49514.618418	32.405722
655.762137	49609.564071	32.410740
656.529593	49686.331344	32.415757
657.019460	49781.719447	32.420775
658.009358	49868.276461	32.425792
658.656002	49953.662018	32.430810
659.164830	50032.962306	32.435828
660.295051	50114.317351	32.440845
660.792290	50194.877291	32.445863
661.494227	50268.139174	32.450880
662.310515	50352.190813	32.455898
662.269145	50440.699239	32.460916
663.333823	50520.339128	32.465933
664.093022	50598.962295	32.470951
664.810782	50691.926171	32.475968
665.765676	50757.081101	32.480986
666.021072	50848.631375	32.486004
667.252716	50924.303393	32.491021
667.394835	51014.312842	32.496039
667.949129	51089.693260	32.501056
669.462484	51171.422101	32.506074
669.729080	51254.008224	32.511092
670.327299	51326.653222	32.516109
670.982873	51413.781004	32.521127
671.448284	51500.403658	32.526144
672.051870	51573.402464	32.531162
672.903781	51665.931863	32.536180
673.404002	51739.959182	32.541197
674.328057	51823.936197	32.546215
674.841279	51909.295581	32.551232
675.477327	51995.816399	32.556250
676.081856	52080.043221	32.561268
676.771688	52152.404490	32.566285
677.678024	52230.157042	32.571303
678.212376	52306.865855	32.576320
679.090513	52382.741024	32.581338
679.440827	52462.766081	32.586356
680.181793	52543.390200	32.591373
680.941972	52618.578215	32.596391
681.105390	52697.131526	32.601408
681.883354	52764.249371	32.606426
682.232263	52853.291745	32.611444
683.136737	52935.033954	32.616461
683.602854	53023.204800	32.621479
684.088844	53110.854688	32.626496
685.321655	53195.051873	32.631514
685.825964	53290.135733	32.636532
686.259792	53380.865984	32.641549
687.176330	53464.996607	32.646567
687.803736	53549.497642	32.651584
688.884275	53636.400763	32.656602
689.209682	53733.569737	32.661620
690.501344	53817.740906	32.666637
690.940259	53904.302766	32.671655
691.708921	53995.827096	32.676672
692.843203	54073.631395	32.681690
693.020530	54161.040070	32.686708
693.799027	54238.158322	32.691725
694.238190	54333.637098	32.696743
694.727548	54415.757418	32.701760
695.600964	54514.602397	32.706778
696.483757	54615.720938	32.711796
696.989278	54706.470707	32.716813
698.022780	54796.286879	32.721831
698.281207	54886.699243	32.726848
699.073673	54976.120132	32.731866
699.597268	55081.401180	32.736884
700.258159	55169.947478	32.741901
701.467670	55261.335242	32.746919
701.772777	55366.597081	32.751936
702.937557	55461.481047	32.756954
703.199993	55554.151551	32.761972
703.999998	55650.581655	32.766989
705.172930	55750.255240	32.772007
705.479774	55838.983148	32.777024
706.686991	55936.787959	32.782042
707.134538	56021.063923	32.787060
707.792901	56126.126014	32.792077
709.036112	56209.569762	32.797095
709.681721	56291.103301	32.802112
710.881714	56381.670021	32.807130
711.026277	56465.979031	32.812148
711.658319	56553.367256	32.817165
712.867633	56638.151717	32.822183
712.971841	56725.065616	32.827200
713.750875	56818.162066	32.832218
714.360261	56913.663000	32.837236
714.973876	57006.117864	32.842253
715.739772	57100.740718	32.847271
716.452764	57197.470745	32.852288
717.458930	57293.236455	32.857306
718.082039	57387.321871	32.862324
718.578251	57477.573954	32.867341
719.492302	57566.569291	32.872359
720.249944	57658.377730	32.877376
720.664420	57751.235496	32.882394
721.236981	57843.391366	32.887412
721.915968	57939.536574	32.892429
722.695662	58035.861488	32.897447
723.149931	58141.220700	32.902464
724.235091	58236.857777	32.907482
724.550327	58323.174931	32.912500
725.830147	58430.377117	32.917517
726.443346	58508.499827	32.922535
726.927593	58605.887480	32.927552
728.006077	58683.845428	32.932570
728.707449	58779.554889	32.937588
729.158786	58862.350724	32.942605
730.119014	58950.744176	32.947623
730.827631	59050.207655	32.952640
731.883244	59122.868788	32.957658
732.347060	59216.047453	32.962676
732.745971	59309.186724	32.967693
733.830511	59403.306351	32.972711
734.354864	59506.834648	32.977728
735.143925	59592.105577	32.982746
735.859787	59691.027492	32.987764
736.056221	59782.856276	32.992781
737.166075	59876.891757	32.997799
737.605886	59977.832586	33.002816
738.388390	60083.943957	33.007834
739.316429	60183.281901	33.012852
739.882956	60286.130943	33.017869
741.037690	60377.639573	33.022887
741.894249	60484.518169	33.027904
742.845773	60576.301476	33.032922
743.106815	60666.246445	33.037940
743.934384	60768.113019	33.042957
745.111490	60868.645572	33.047975
745.342750	60964.525270	33.052992
746.418379	61058.205295	33.058010
747.374877	61173.211657	33.063028
747.854453	61268.185805	33.068045
748.965243	61347.014555	33.073063
749.411302	61461.582373	33.078080
750.018836	61564.115047	33.083098
750.989908	61667.314969	33.088116
751.729912	61758.892079	33.093133
752.749816	61847.958246	33.098151
753.099163	61965.085777	33.103168
753.933778	62053.001516	33.108186
754.574074	62154.880692	33.113204
755.447651	62270.172403	33.118221
756.553179	62361.375702	33.123239
756.946043	62473.543420	33.128256
757.518231	62567.440041	33.133274
758.596776	62671.872450	33.138292
759.261952	62764.724283	33.143309
760.228394	62868.790658	33.148327
760.851682	62971.201329	33.153344
761.697187	63082.842380	33.158362
762.366950	63177.566339	33.163380
763.086984	63288.287417	33.168397
764.076197	63384.609291	33.173415
764.705693	63491.079675	33.178432
765.293384	63585.534627	33.183450
766.067769	63690.888509	33.188468
766.909017	63796.383577	33.193485
767.756612	63893.230623	33.198503
768.156376	64006.511746	33.203520
769.054256	64112.302478	33.208538
770.304059	64209.229864	33.213556
770.650065	64319.809719	33.218573
771.517897	64416.428291	33.223591
772.266259	64529.098317	33.228608
772.792087	64627.405379	33.233626
773.722166	64734.376075	33.238644
774.411004	64842.044666	33.243661
775.211033	64948.620751	33.248679
775.504964	65064.036552	33.253696
776.618873	65155.244464	33.258714
777.603199	65255.425722	33.263732
777.888793	65363.960240	33.268749
778.845497	65460.720678	33.273767
779.740902	65573.719726	33.278784
780.291580	65675.062072	33.283802
781.183997	65773.718495	33.288820
781.691418	65870.201119	33.293837
782.740596	65982.747054	33.298855
783.411263	66098.649934	33.303872
783.909155	66206.382425	33.308890
784.946080	66315.271747	33.313908
785.340112	66427.555434	33.318925
785.944183	66538.603784	33.323943
786.589925	66658.370344	33.328960
787.626880	66785.166329	33.333978
788.527391	66892.431124	33.338996
789.060257	67021.132699	33.344013
790.054345	67141.533511	33.349031
790.583074	67255.228162	33.354048
791.354913	67387.685821	33.359066
792.156354	67506.185946	33.364084
793.225310	67634.644530	33.369101
794.132724	67749.265500	33.374119
794.919651	67872.815388	33.379136
795.508990	68002.247005	33.384154
796.690797	68122.350490	33.389172
797.383879	68250.641050	33.394189
798.304399	68367.046165	33.399207
799.257363	68500.239543	33.404224
800.173587	68615.970209	33.409242
800.808885	68726.373650	33.414260
801.583737	68859.630353	33.419277
802.590843	68968.437120	33.424295
803.509607	69088.033168	33.429312
804.178756	69202.062786	33.434330
805.021231	69329.715504	33.439348
805.718262	69458.644986	33.444365
806.633681	69569.575528	33.449383
807.713420	69690.817599	33.454400
808.538410	69813.303873	33.459418
809.452233	69920.436347	33.464436
810.023409	70044.831236	33.469453
810.885262	70152.776505	33.474471
811.681571	70274.252133	33.479488
812.705347	70405.599321	33.484506
813.765024	70512.489319	33.489524
814.752377	70627.820760	33.494541
815.462065	70734.605346	33.499559
816.207074	70849.497487	33.504576
816.796096	70973.142324	33.509594
818.010618	71071.302181	33.514612
818.308252	71195.502362	33.519629
819.119697	71297.467082	33.524647
819.887583	71424.303580	33.529664
820.745752	71549.601912	33.534682
821.426409	71667.285101	33.539700
822.161578	71784.327550	33.544717
823.222039	71912.541342	33.549735
823.679403	72029.555182	33.554752
824.151111	72161.971911	33.559770
825.083541	72279.313246	33.564788
825.659045	72407.490025	33.569805
826.620944	72537.020195	33.574823
827.298347	72683.685347	33.579840
828.116312	72813.942927	33.584858
829.425525	72947.244079	33.589876
830.059569	73076.869636	33.594893
830.642375	73190.333860	33.599911
831.762024	73319.880548	33.604928
832.560354	73442.790235	33.609946
833.587696	73560.470613	33.614964
833.924649	73684.058761	33.619981
834.779101	73789.183844	33.624999
835.824933	73915.369145	33.630016
836.272520	74049.502561	33.635034
837.116440	74175.887190	33.640052
837.867041	74305.848599	33.645069
838.947683	74435.832084	33.650087
839.648421	74567.561474	33.655104
840.229048	74712.080640	33.660122
841.453185	74845.742641	33.665140
842.134140	74977.370242	33.670157
843.115309	75115.166054	33.675175
843.456739	75233.930197	33.680192
844.803440	75377.549101	33.685210
845.772950	75509.505313	33.690228
846.201148	75657.857042	33.695245
847.488056	75796.220044	33.700263
848.477672	75930.876134	33.705280
848.942897	76075.328445	33.710298
849.672224	76201.598179	33.715316
850.526640	76356.544226	33.720333
851.465331	76492.508767	33.725351
852.555240	76622.370780	33.730368
853.394932	76769.074310	33.735386
854.116047	76902.376540	33.740404
854.944800	77053.182422	33.745421
856.082648	77186.012619	33.750439
857.130473	77326.056604	33.755456
858.001179	77477.041848	33.760474
859.138990	77603.878188	33.765492
859.801578	77752.578328	33.770509
860.152412	77880.855743	33.775527
861.737335	78023.345426	33.780544
862.239626	78166.622314	33.785562
863.475060	78292.409040	33.790580
864.108903	78425.614611	33.795597
865.226381	78568.602558	33.800615
866.045092	78703.980507	33.805632
866.502482	78850.792555	33.810650
867.503121	78978.709425	33.815668
868.370144	79123.361700	33.820685
869.436265	79265.439015	33.825703
870.117121	79408.308411	33.830720
870.939549	79555.229147	33.835738
872.172359	79685.420568	33.840756
872.748997	79831.390585	33.845773
873.838290	79964.985399	33.850791
874.772605	80105.407090	33.855808
875.619780	80254.580335	33.860826
876.334524	80383.937852	33.865844
877.575179	80522.805857	33.870861
878.104546	80664.057113	33.875879
879.424749	80796.422994	33.880896
880.310208	80942.393369	33.885914
881.204374	81074.698478	33.890932
882.209160	81217.778755	33.895949
882.923161	81344.149509	33.900967
883.485043	81470.432245	33.905984
884.244445	81617.851229	33.911002
885.314807	81758.001238	33.916020
886.163532	81901.238137	33.921037
887.435805	82041.963839	33.926055
888.534996	82161.366823	33.931072
888.936504	82303.294676	33.936090
890.060147	82423.296009	33.941108
890.875022	82552.851713	33.946125
891.732707	82678.718916	33.951143
892.563323	82798.530256	33.956160
893.209457	82925.003201	33.961178
894.020839	83053.632266	33.966196
894.890201	83186.175112	33.971213
895.702247	83320.379520	33.976231
896.762717	83455.625529	33.981248
897.218464	83596.761516	33.986266
898.360951	83727.699542	33.991284
899.215783	83867.404548	33.996301
899.632756	84009.492194	34.001319
900.759945	84146.502793	34.006336
901.506061	84301.381855	34.011354
902.464173	84454.379347	34.016372
903.759194	84590.795367	34.021389
904.440941	84736.893113	34.026407
905.343887	84895.995807	34.031424
906.086855	85041.908176	34.036442
907.330046	85190.282351	34.041460
907.831392	85335.091252	34.046477
908.917796	85487.068248	34.051495
910.305997	85637.091739	34.056512
910.601466	85794.212933	34.061530
911.419858	85937.353273	34.066548
912.663706	86084.480150	34.071565
913.589242	86247.872129	34.076583
914.803257	86396.986467	34.081600
915.559802	86557.637001	34.086618
916.559029	86699.410595	34.091636
917.590296	86857.511931	34.096653
918.377397	87021.697849	34.101671
919.263916	87168.188204	34.106688
919.711193	87323.396124	34.111706
920.799584	87484.029731	34.116724
922.004359	87632.659831	34.121741
922.768858	87796.854872	34.126759
923.693165	87947.634261	34.131776
924.455836	88112.850624	34.136794
925.495510	88277.680603	34.141812
926.435596	88436.130306	34.146829
927.105434	88606.206581	34.151847
928.049893	88763.493329	34.156864
929.004332	88931.936446	34.161882
929.911400	89094.800562	34.166900
930.853481	89257.641014	34.171917
931.859990	89434.831375	34.176935
932.762762	89585.814551	34.181952
933.943164	89765.275876	34.186970
934.802810	89927.963647	34.191988
935.619355	90086.767489	34.197005
936.323631	90262.716561	34.202023
937.538016	90425.652820	34.207040
938.392954	90599.990914	34.212058
939.496720	90763.011036	34.217076
940.155796	90927.226019	34.222093
941.047269	91096.049156	34.227111
942.294559	91271.820860	34.232128
942.967423	91446.239474	34.237146
944.166600	91609.236869	34.242164
945.015112	91783.122533	34.247181
945.863290	91951.433471	34.252199
946.942427	92115.656667	34.257216
947.594288	92299.028102	34.262234
948.799529	92460.903595	34.267252
949.736555	92634.476899	34.272269
950.679340	92805.100975	34.277287
951.781407	92951.616297	34.282304
952.568014	93115.242665	34.287322
953.250728	93278.020159	34.292340
954.401114	93437.537618	34.297357
955.110549	93606.939954	34.302375
956.025800	93766.631357	34.307392
956.882078	93934.948289	34.312410
957.725364	94104.534472	34.317428
958.735669	94278.987140	34.322445
959.344793	94451.424864	34.327463
960.389291	94627.754309	34.332480
961.264287	94803.315470	34.337498
962.317409	94986.305141	34.342516
963.192955	95162.811929	34.347533
963.873807	95356.848496	34.352551
964.768327	95538.906301	34.357568
965.953683	95723.759593	34.362586
966.919637	95919.361271	34.367604
968.086771	96095.484636	34.372621
968.851513	96286.292475	34.377639
970.018701	96465.241762	34.382656
971.110202	96669.323903	34.387674
971.715631	96858.181032	34.392692
972.994284	97037.464157	34.397709
973.961414	97228.473611	34.402727
975.105973	97418.220712	34.407744
976.411671	97612.886836	34.412762
977.248630	97799.288118	34.417780
978.330544	97988.821976	34.422797
979.417446	98175.456931	34.427815
980.354588	98361.662210	34.432832
981.316357	98543.249574	34.437850
982.228757	98731.873734	34.442868
983.490162	98915.478102	34.447885
984.131951	99104.289060	34.452903
985.191567	99295.963614	34.457920
986.425292	99481.172078	34.462938
987.286113	99676.054255	34.467956
988.465456	99867.738640	34.472973
989.374795	100058.348479	34.477991
990.134622	100234.194536	34.483008
991.398996	100429.750164	34.488026
992.172999	100618.423833	34.493044
993.327468	100803.794279	34.498061
994.527360	101007.842779	34.503079
995.414374	101192.760067	34.508096
996.670911	101376.705834	34.513114
997.233111	101573.076411	34.518132
998.563604	101762.768156	34.523149
999.531971	101953.774853	34.528167
1000.609729	102140.250320	34.533184
1001.564725	102329.425786	34.538202
1002.584100	102520.738488	34.543220
1003.895023	102708.426863	34.548237
1004.548163	102899.739593	34.553255
1005.839673	103088.826952	34.558272
1006.676371	103277.819922	34.563290
1007.197269	103476.421606	34.568308
1008.573272	103667.006223	34.573325
1009.004652	103859.432783	34.578343
1010.079949	104053.755270	34.583360
1011.351618	104250.706284	34.588378
1012.030660	104457.153943	34.593396
1013.131639	104647.854485	34.598413
1014.052248	104844.070111	34.603431
1015.059363	105059.865565	34.608448
1015.862298	105251.063023	34.613466
1016.914553	105464.030009	34.618484
1018.226596	105650.384079	34.623501
1018.811728	105851.095478	34.628519
1020.224006	106031.280302	34.633536
1021.251803	106212.441837	34.638554
1022.073285	106414.055653	34.643572
1023.569614	106597.713457	34.648589
1024.257367	106791.220869	34.653607
1025.119186	106987.196076	34.658624
1026.477114	107176.580387	34.663642
1027.250524	107376.714833	34.668660
1028.251842	107569.707381	34.673677
1029.052488	107775.388067	34.678695
1030.096770	107973.822897	34.683712
1031.280337	108177.758722	34.688730
1031.694941	108386.750512	34.693748
1032.874482	108591.678120	34.698765
1034.150758	108799.428632	34.703783
1035.036016	109017.366180	34.708800
1036.102842	109228.992665	34.713818
1036.823034	109442.527497	34.718836
1038.238412	109648.095447	34.723853
1039.305916	109867.707074	34.728871
1040.443313	110079.366504	34.733888
1041.645464	110285.810562	34.738906
1042.290706	110507.726616	34.743924
1043.385944	110722.792889	34.748941
1044.831929	110950.204549	34.753959
1045.840056	111159.600843	34.758976
1046.639601	111372.960269	34.763994
1047.505987	111589.641982	34.769012
1048.714081	111806.408247	34.774029
1049.880823	112032.228153	34.779047
1051.208490	112258.922745	34.784064
1052.182197	112473.414685	34.789082
1053.207773	112701.898416	34.794100
1054.608065	112912.776031	34.799117
1055.560256	113133.294210	34.804135
1056.363120	113353.978179	34.809152
1057.935701	113562.982577	34.814170
1058.734421	113784.354748	34.819188
1059.660031	114009.926502	34.824205
1060.696889	114232.060987	34.829223
1061.955374	114450.157082	34.834240
1063.280974	114663.404056	34.839258
1063.992732	114895.796403	34.844276
1065.292452	115110.051923	34.849293
1066.211364	115326.842620	34.854311
1067.315505	115553.474127	34.859328
1068.460945	115771.168334	34.864346
1069.578874	115989.438908	34.869364
1070.782848	116206.645311	34.874381
1071.794423	116429.941532	34.879399
1072.589995	116652.844422	34.884416
1074.071885	116863.180584	34.889434
1074.940863	117093.677004	34.894452
1076.460799	117306.683605	34.899469
1077.267822	117524.143027	34.904487
1078.254000	117742.385400	34.909504
1079.629814	117951.125210	34.914522
1080.833307	118171.755039	34.919540
1081.902977	118380.890688	34.924557
1083.047932	118608.718016	34.929575
1083.724984	118822.115912	34.934592
1084.968005	119033.331032	34.939610
1085.898276	119252.595068	34.944628
1087.321901	119465.962955	34.949645
1088.598224	119694.828808	34.954663
1089.243966	119910.254636	34.959680
1090.469219	120112.470915	34.964698
1091.332799	120319.082173	34.969716
1092.542079	120517.629037	34.974733
1093.615338	120728.757751	34.979751
1094.548014	120934.044010	34.984768
1095.636993	121136.530635	34.989786
1096.562583	121356.824949	34.994804
1097.478071	121556.998753	34.999821
1098.238272	121779.693300	35.004839
1099.106515	122008.657273	35.009856
1100.622539	122228.860449	35.014874
1101.302312	122459.519175	35.019892
1102.793284	122688.613533	35.024909
1104.089624	122904.283097	35.029927
1105.060453	123139.740040	35.034944
1106.391014	123359.551329	35.039962
1107.205254	123601.868636	35.044980
1108.474211	123828.701873	35.049997
1109.658828	124047.680529	35.055015
1110.876843	124278.289594	35.060032
1111.931791	124497.014125	35.065050
1112.587118	124738.023413	35.070068
1114.226323	124968.403341	35.075085
1115.318737	125196.948971	35.080103
1115.895669	125435.454629	35.085120
1117.494126	125673.590483	35.090138
1118.632993	125913.895426	35.095156
1119.600290	126142.836374	35.100173
1121.037907	126373.843259	35.105191
1122.102556	126617.195176	35.110208
1123.254962	126841.776034	35.115226
1124.343693	127097.739036	35.120244
1125.626394	127330.844692	35.125261
1126.803834	127565.249676	35.130279
1128.215535	127809.250729	35.135296
1129.079507	128031.669776	35.140314
1130.337938	128273.228161	35.145332
1131.479006	128506.911094	35.150349
1132.676781	128746.264988	35.155367
1133.534912	128988.642932	35.160384
1134.787773	129219.055095	35.165402
1136.195609	129464.223200	35.170420
1137.105673	129693.225127	35.175437
1138.265611	129932.163337	35.180455
1139.632243	130171.411436	35.185472
1140.900927	130401.347939	35.190490
1141.943618	130641.477089	35.195508
1143.147614	130882.608166	35.200525
1144.640534	131113.184597	35.205543
1145.469553	131348.144416	35.210560
1146.694185	131576.981171	35.215578
1147.444048	131813.123736	35.220596
1148.929698	132041.071322	35.225613
1150.144150	132279.282882	35.230631
1151.261484	132530.328630	35.235648
1152.648414	132755.293167	35.240666
1153.818546	132995.824566	35.245684
1154.980579	133232.200969	35.250701
1155.795973	133459.432686	35.255719
1156.696974	133705.896106	35.260736
1157.874760	133934.161487	35.265754
1159.005762	134178.308514	35.270772
1160.500020	134427.962809	35.275789
1162.057982	134671.586541	35.280807
1162.763010	134908.266164	35.285824
1163.812791	135134.697434	35.290842
1165.414241	135380.499840	35.295860
1166.415487	135612.165765	35.300877
1167.463426	135827.876408	35.305895
1168.463971	136068.166821	35.310912
1169.934088	136283.404935	35.315930
1170.736259	136513.005453	35.320948
1171.646574	136738.291647	35.325965
1173.075134	136970.023191	35.330983
1173.725311	137207.527049	35.336000
1175.205181	137429.325849	35.341018
1176.364045	137678.717756	35.346036
1177.101224	137919.901834	35.351053
1178.443148	138149.513095	35.356071
1179.780061	138395.799860	35.361088
1180.761503	138641.830199	35.366106
1181.462272	138891.053201	35.371124
1182.592414	139143.376917	35.376141
1184.060759	139384.222323	35.381159
1185.158660	139655.587164	35.386176
1185.934522	139914.682681	35.391194
1187.106304	140167.742506	35.396212
1188.588521	140432.481814	35.401229
1189.716714	140688.570503	35.406247
1190.856098	140956.274235	35.411264
1192.034486	141223.212779	35.416282
1193.708422	141493.558552	35.421300
1194.606468	141761.333759	35.426317
1196.116192	142017.648171	35.431335
1197.138904	142285.482880	35.436352
1198.429733	142551.728272	35.441370
1199.782815	142816.405658	35.446388
1200.883617	143088.304130	35.451405
1201.833101	143358.441692	35.456423
1203.083789	143636.558665	35.461440
1204.354147	143905.747012	35.466458
1205.649498	144171.420554	35.471476
1206.786010	144448.091735	35.476493
1208.202078	144725.847504	35.481511
1209.063893	144989.062509	35.486528
1210.519855	145273.397675	35.491546
1211.676357	145548.805897	35.496564
1212.662310	145824.700965	35.501581
1214.519540	146097.702135	35.506599
1215.781010	146376.586867	35.511616
1216.747746	146651.958775	35.516634
1218.071803	146923.177336	35.521652
1219.184029	147203.107660	35.526669
1220.615214	147473.716535	35.531687
1221.685480	147750.018119	35.536704
1223.203630	148024.015604	35.541722
1224.623377	148302.470352	35.546740
1225.400973	148576.150458	35.551757
1227.322260	148853.524515	35.556775
1228.158343	149126.311214	35.561792
1229.615775	149392.275162	35.566810
1230.839607	149669.263271	35.571828
1231.760521	149952.366118	35.576845
1233.109589	150215.436681	35.581863
1234.001281	150502.480359	35.586880
1235.344202	150777.465660	35.591898
1236.594854	151055.220572	35.596916
1238.189871	151343.473491	35.601933
1238.919435	151608.127477	35.606951
1240.394996	151891.812749	35.611968
1241.749559	152177.257843	35.616986
1242.974418	152442.825107	35.622004
1243.928719	152734.695265	35.627021
1245.735717	152999.041257	35.632039
1246.457762	153281.174345	35.637056
1247.555977	153561.585645	35.642074
1249.084617	153825.894514	35.647092
1250.096868	154102.493188	35.652109
1251.499818	154356.019096	35.657127
1252.630703	154620.779647	35.662144
1253.967869	154905.803780	35.667162
1254.849197	155165.915837	35.672180
1256.077872	155449.553807	35.677197
1257.116195	155703.503870	35.682215
1258.645027	155984.292640	35.687232
1259.893430	156276.774919	35.692250
1261.662673	156547.912427	35.697268
1262.426452	156835.569638	35.702285
1263.792004	157110.875125	35.707303
1264.845938	157387.007836	35.712320
1266.191737	157676.147903	35.717338
1267.504616	157965.346227	35.722356
1268.707789	158244.859965	35.727373
1269.994175	158529.372877	35.732391
1270.962996	158824.825002	35.737408
1272.070896	159112.137069	35.742426
1273.616193	159406.673511	35.747444
1274.955555	159712.841515	35.752461
1276.262959	160004.846214	35.757479
1277.689489	160309.646782	35.762496
1278.894449	160597.346455	35.767514
1280.141314	160889.392767	35.772532
1281.211491	161210.459899	35.777549
1282.895221	161493.417843	35.782567
1284.235261	161800.704887	35.787584
1285.401221	162113.871736	35.792602
1286.806022	162403.098619	35.797620
1287.888343	162708.176533	35.802637
1289.514638	163015.107909	35.807655
1290.670068	163319.175812	35.812672
1291.680410	163622.749665	35.817690
1293.339594	163927.436447	35.822708
1294.314619	164251.079863	35.827725
1295.944296	164544.331478	35.832743
1297.428677	164848.888715	35.837760
1298.221234	165167.608133	35.842778
1300.000987	165467.058333	35.847796
1301.018508	165780.174934	35.852813
1302.375154	166089.786487	35.857831
1303.527896	166390.552014	35.862848
1304.952944	166712.159891	35.867866
1306.694145	167011.068672	35.872884
1307.676526	167336.002513	35.877901
1308.900454	167634.468044	35.882919
1310.640138	167948.432259	35.887936
1311.508704	168270.688960	35.892954
1313.382055	168580.232420	35.897972
1314.641220	168890.894639	35.902989
1315.839810	169205.045842	35.908007
1317.468193	169512.682005	35.913024
1318.800523	169828.236597	35.918042
1320.201808	170130.775237	35.923060
1321.194810	170432.228592	35.928077
1322.644084	170742.783122	35.933095
1324.172537	171049.405517	35.938112
1325.431872	171353.942521	35.943130
1326.969521	171662.737390	35.948148
1328.104963	171975.585422	35.953165
1329.213789	172273.376821	35.958183
1330.369457	172577.126726	35.963200
1331.938083	172900.251767	35.968218
1333.873346	173202.633190	35.973236
1334.759573	173506.243206	35.978253
1336.351547	173804.586176	35.983271
1337.565500	174095.112639	35.988288
1338.587633	174384.505017	35.993306
1340.332910	174665.505275	35.998324
1341.608587	174958.196830	36.003341
1342.759660	175243.296224	36.008359
1343.916995	175534.982837	36.013376
1344.768776	175833.156019	36.018394
1346.520079	176128.187251	36.023412
1347.584728	176432.039860	36.028429
1348.917728	176731.852241	36.033447
1349.949367	177035.802834	36.038464
1351.246081	177352.808983	36.043482
1352.840101	177659.018325	36.048500
1354.178464	177986.999712	36.053517
1355.631545	178280.189203	36.058535
1356.854191	178608.079511	36.063552
1358.016641	178928.658715	36.068570
1359.523277	179249.018051	36.073588
1360.699408	179572.835448	36.078605
1361.987102	179900.532891	36.083623
1363.380030	180213.758709	36.088640
1364.642274	180552.671602	36.093658
1366.298577	180871.074334	36.098676
1367.453123	181204.158111	36.103693
1368.640098	181533.659372	36.108711
1370.163861	181875.469524	36.113728
1371.593965	182209.351796	36.118746
1372.860558	182545.649398	36.123764
1374.429283	182889.679832	36.128781
1376.007707	183223.378902	36.133799
1377.584089	183557.550007	36.138816
1378.572209	183898.547661	36.143834
1380.101754	184237.147833	36.148852
1381.199380	184564.537277	36.153869
1382.969715	184915.274552	36.158887
1384.385226	185259.345242	36.163904
1385.605362	185605.658995	36.168922
1387.239507	185944.683905	36.173940
1388.710391	186286.048064	36.178957
1390.260055	186626.144605	36.183975
1392.037803	186976.347745	36.188992
1393.033312	187320.297349	36.194010
1394.609680	187652.296992	36.199028
1396.121020	188000.760600	36.204045
1397.472577	188333.423320	36.209063
1399.074891	188675.427414	36.214080
1400.282528	189005.782056	36.219098
1402.103946	189337.649295	36.224116
1402.963610	189676.684574	36.229133
1404.546686	190028.093483	36.234151
1406.444655	190358.608199	36.239168
1407.689402	190698.385414	36.244186
1408.828099	191024.065727	36.249204
1410.288938	191372.087885	36.254221
1411.813928	191708.650819	36.259239
1413.597354	192033.239823	36.264256
1414.674798	192379.985445	36.269274
1415.958606	192707.212235	36.274292
1417.327146	193050.917523	36.279309
1418.608642	193396.467181	36.284327
1420.447476	193734.042981	36.289344
1421.652013	194070.836748	36.294362
1423.183481	194416.896599	36.299380
1424.335368	194756.940000	36.304397
1425.665837	195103.988945	36.309415
1427.131269	195441.394308	36.314432
1428.604142	195793.336576	36.319450
1429.885917	196127.944762	36.324468
1431.010825	196462.758324	36.329485
1432.432494	196794.210973	36.334503
1434.214469	197122.685718	36.339520
1435.090335	197457.799395	36.344538
1436.483330	197798.174279	36.349556
1438.180922	198131.492380	36.354573
1440.063554	198456.770357	36.359591
1441.078998	198791.575603	36.364608
1442.157848	199149.517112	36.369626
1443.217424	199483.848694	36.374644
1445.327124	199833.789854	36.379661
1446.015659	200181.275987	36.384679
1447.557878	200545.293177	36.389696
1449.113235	200896.423154	36.394714
1450.639123	201252.574878	36.399732
1452.110305	201621.573695	36.404749
1452.972466	201992.147862	36.409767
1454.648548	202354.590496	36.414784
1456.196370	202714.326323	36.419802
1457.958703	203079.132616	36.424820
1459.272506	203447.608065	36.429837
1460.388889	203821.679251	36.434855
1462.302162	204196.052339	36.439872
1463.563705	204555.501602	36.444890
1465.141283	204931.381289	36.449908
1466.776820	205312.408338	36.454925
1468.602356	205692.999574	36.459943
1470.451005	206058.136178	36.464960
1471.831332	206431.440140	36.469978
1473.105150	206808.471149	36.474996
1475.046422	207165.801365	36.480013
1475.927345	207543.434093	36.485031
1477.398569	207913.555634	36.490048
1478.564655	208299.918887	36.495066
1480.014159	208678.643877	36.500084
1481.711580	209059.970809	36.505101
1483.177426	209447.661322	36.510119
1484.992714	209823.778860	36.515136
1486.100833	210211.316168	36.520154
1487.796564	210595.482062	36.525172
1489.460689	210982.397710	36.530189
1490.436514	211371.638318	36.535207
1492.526031	211746.449234	36.540224
1493.862670	212151.176370	36.545242
1495.356020	212521.670104	36.550260
1497.267697	212919.854990	36.555277
1498.489099	213304.263582	36.560295
1500.609623	213678.493424	36.565312
1501.705346	214077.503966	36.570330
1503.220942	214456.865586	36.575348
1504.943059	214841.807456	36.580365
1506.244383	215231.671356	36.585383
1508.044975	215603.472903	36.590400
1509.183459	215993.900201	36.595418
1510.580417	216381.086263	36.600436
1512.319620	216768.496705	36.605453
1513.607602	217151.157625	36.610471
1515.684534	217537.524786	36.615488
1517.066431	217930.230836	36.620506
1518.325101	218310.869209	36.625524
1520.572322	218703.282909	36.630541
1521.803198	219085.528867	36.635559
1523.150699	219468.468129	36.640576
1524.464677	219857.002037	36.645594
1525.983926	220236.004335	36.650612
1527.391001	220622.239783	36.655629
1529.091686	221020.746582	36.660647
1530.676336	221406.091930	36.665664
1531.604665	221779.279305	36.670682
1533.008847	222151.982928	36.675700
1535.203332	222515.362686	36.680717
1536.401262	222898.135565	36.685735
1538.046383	223256.909581	36.690752
1539.338439	223720.973231	36.695770
1540.821728	224104.871334	36.700788
1542.377213	224479.462468	36.705805
1543.803546	224868.706380	36.710823
1544.976651	225249.738429	36.715840
1546.705177	225644.751461	36.720858
1547.901125	226040.056943	36.725876
1549.805896	226434.103558	36.730893
1550.926272	226839.914269	36.735911
1552.703922	227239.369208	36.740928
1554.259921	227644.831069	36.745946
1555.508088	228042.013703	36.750964
1557.464207	228460.035951	36.755981
1558.656450	228876.788661	36.760999
1560.397394	229269.575385	36.766016
1562.030111	229690.042468	36.771034
1563.172977	230107.899249	36.776052
1565.179524	230521.550421	36.781069
1566.462349	230948.683226	36.786087
1568.388783	231367.836624	36.791104
1569.912044	231780.682134	36.796122
1571.382563	232207.406500	36.801140
1573.156301	232623.007020	36.806157
1574.510308	233054.350571	36.811175
1576.424738	233478.998350	36.816192
1578.041363	233904.001255	36.821210
1579.235750	234337.584504	36.826228
1581.393492	234756.530838	36.831245
1583.064889	235195.143181	36.836263
1584.557840	235612.270897	36.841280
1586.056256	236045.833605	36.846298
1587.668433	236471.885031	36.851316
1589.147665	236897.654582	36.856333
1590.551379	237333.039490	36.861351
1592.133297	237760.546741	36.866368
1593.899064	238204.967694	36.871386
1595.283825	238661.467757	36.876404
1597.183339	239084.429200	36.881421
1598.670799	239522.065821	36.886439
1600.437945	239967.023778	36.891456
1602.114976	240409.812930	36.896474
1603.722776	240845.247718	36.901492
1605.432102	241281.555641	36.906509
1607.028442	241732.565637	36.911527
1608.614892	242171.080093	36.916544
1610.103757	242604.937381	36.921562
1611.553594	243057.777563	36.926580
1613.414839	243490.406300	36.931597
1614.587900	243943.623945	36.936615
1616.391619	244386.297641	36.941632
1617.937163	244838.261258	36.946650
1619.375880	245298.753135	36.951668
1621.137062	245743.112464	36.956685
1622.921147	246207.003407	36.961703
1624.366854	246644.862162	36.966720
1626.226945	247099.139501	36.971738
1628.178338	247553.884996	36.976756
1629.420134	247994.878258	36.981773
1630.976534	248453.856174	36.986791
1632.706591	248905.185022	36.991808
1634.509560	249356.527712	36.996826
1635.808240	249811.205762	37.001844
1637.776917	250253.249854	37.006861
1639.117512	250695.474311	37.011879
1640.570409	251128.992723	37.016896
1642.508570	251560.780113	37.021914
1644.241884	251992.881098	37.026932
1646.138578	252430.112244	37.031949
1647.427209	252861.398165	37.036967
1648.629471	253301.716756	37.041984
1650.465619	253744.572823	37.047002
1652.038112	254184.881546	37.052020
1654.114335	254621.449199	37.057037
1655.441736	255060.935095	37.062055
1656.666116	255509.557953	37.067072
1658.720209	255955.605189	37.072090
1660.512152	256408.580150	37.077108
1662.021701	256862.973648	37.082125
1663.859450	257319.472300	37.087143
1665.502685	257777.679767	37.092160
1667.131340	258228.116274	37.097178
1668.787713	258691.986570	37.102196
1670.500239	259151.274992	37.107213
1672.041131	259611.303029	37.112231
1673.715512	260068.844844	37.117248
1675.372039	260529.209298	37.122266
1677.113457	261001.804016	37.127284
1679.362628	261469.640526	37.132301
1680.843316	261934.479222	37.137319
1682.531303	262407.285527	37.142336
1684.429382	262867.761748	37.147354
1686.175705	263328.618461	37.152372
1687.964421	263786.902201	37.157389
1689.456870	264267.106772	37.162407
1691.106390	264729.274219	37.167424
1692.874798	265202.776925	37.172442
1694.385287	265669.818665	37.177460
1696.901848	266141.063185	37.182477
1698.426175	266607.670004	37.187495
1699.668319	267074.577039	37.192512
1701.627866	267551.119896	37.197530
1703.324127	268028.696463	37.202548
1705.251402	268494.980817	37.207565
1706.896769	268972.132875	37.212583
1708.521690	269446.671230	37.217600
1710.345914	269914.774535	37.222618
1712.138810	270395.710859	37.227636
1713.918806	270869.205616	37.232653
1715.963658	271343.545050	37.237671
1717.289572	271822.803655	37.242688
1719.455481	272289.856479	37.247706
1720.954911	272771.066340	37.252724
1722.866713	273247.355382	37.257741
1724.068340	273717.003822	37.262759
1725.761098	274198.255498	37.267776
1727.604336	274662.741186	37.272794
1728.958900	275153.877709	37.277812
1730.919606	275639.299207	37.282829
1732.754236	276117.297658	37.287847
1734.443482	276597.402132	37.292864
1736.135850	277081.290009	37.297882
1738.038705	277570.781346	37.302900
1739.556687	278054.060815	37.307917
1741.500362	278539.910677	37.312935
1743.193481	279023.514589	37.317952
1745.051271	279505.845440	37.322970
1746.073798	280004.976693	37.327988
1747.988734	280484.603061	37.333005
1749.887627	280987.803671	37.338023
1751.377436	281479.385689	37.343040
1753.427382	281958.274640	37.348058
1755.058907	282436.723358	37.353076
1756.798796	282898.692692	37.358093
1758.477806	283369.485096	37.363111
1759.856722	283847.158678	37.368128
1762.124986	284304.616976	37.373146
1763.743811	284787.506192	37.378164
1765.349194	285271.081963	37.383181
1767.228578	285754.737959	37.388199
1768.635045	286229.580182	37.393216
1770.758456	286713.726184	37.398234
1772.337527	287205.656907	37.403252
1773.799969	287689.781792	37.408269
1775.469289	288168.079505	37.413287
1776.924794	288681.184157	37.418304
1778.805982	289188.603077	37.423322
1780.387795	289695.332904	37.428340
1782.539219	290198.283673	37.433357
1784.555161	290709.535294	37.438375
1785.917118	291227.166670	37.443392
1787.824541	291737.085852	37.448410
1789.566515	292267.934272	37.453428
1791.625224	292781.837278	37.458445
1793.330704	293287.617751	37.463463
1794.649103	293828.028636	37.468480
1796.821071	294339.569386	37.473498
1798.760858	294865.801542	37.478516
1800.530785	295403.158698	37.483533
1802.219174	295929.732155	37.488551
1803.942023	296461.631146	37.493568
1806.108542	296987.002966	37.498586
1807.922022	297534.298689	37.503604
1809.760688	298071.097832	37.508621
1811.540616	298595.001539	37.513639
1813.252491	299134.152717	37.518656
1815.266086	299665.225394	37.523674
1816.932628	300212.327847	37.528692
1818.881274	300747.215123	37.533709
1820.928596	301291.480278	37.538727
1822.298482	301835.320866	37.543744
1824.508113	302381.584775	37.548762
1826.213027	302931.001897	37.553780
1828.355818	303472.927493	37.558797
1829.942946	304019.792433	37.563815
1831.572622	304576.780320	37.568832
1833.576884	305123.315653	37.573850
1835.544750	305673.307507	37.578868
1836.876368	306220.683547	37.583885
1838.831378	306777.222719	37.588903
1840.915071	307343.742979	37.593920
1842.767088	307893.942804	37.598938
1844.688460	308453.549283	37.603956
1846.607641	309004.416280	37.608973
1848.611275	309561.919136	37.613991
1850.251013	310126.665007	37.619008
1851.914252	310684.114645	37.624026
1854.275018	311251.171296	37.629044
1855.846941	311804.844193	37.634061
1857.804818	312358.296994	37.639079
1859.524008	312921.434950	37.644096
1861.629171	313482.067130	37.649114
1863.242088	314053.670291	37.654132
1865.463990	314611.582899	37.659149
1867.236559	315158.697079	37.664167
1869.071135	315727.838140	37.669184
1870.729576	316294.845354	37.674202
1872.638389	316859.165833	37.679220
1874.452676	317427.077726	37.684237
1876.505452	317979.481652	37.689255
1878.047658	318528.004278	37.694272
1879.583457	319067.610975	37.699290
1881.546791	319614.023919	37.704308
1883.333671	320159.293529	37.709325
1885.199988	320712.924671	37.714343
1886.948843	321270.963206	37.719360
1888.918283	321818.626446	37.724378
1890.907334	322384.486907	37.729396
1892.359288	322947.460375	37.734413
1894.283517	323514.032440	37.739431
1896.176431	324083.651368	37.744448
1898.246330	324644.958808	37.749466
1899.674407	325213.095354	37.754484
1901.320353	325797.211287	37.759501
1902.992206	326382.662943	37.764519
1905.151251	326980.418179	37.769536
1907.069104	327567.417135	37.774554
1909.152082	328157.607312	37.779572
1910.640969	328764.137974	37.784589
1912.667660	329360.215310	37.789607
1914.427646	329964.200641	37.794624
1916.013689	330563.537070	37.799642
1918.214585	331188.660308	37.804660
1920.240543	331800.959837	37.809677
1921.909527	332430.295063	37.814695
1923.539537	333056.938635	37.819712
1925.992126	333679.479033	37.824730
1927.728310	334303.552181	37.829748
1929.596219	334937.039643	37.834765
1931.928943	335565.873566	37.839783
1933.803021	336200.385754	37.844800
1935.711582	336851.892053	37.849818
1937.740104	337473.061956	37.854836
1939.410717	338112.864332	37.859853
1942.007889	338746.845254	37.864871
1943.426897	339409.086424	37.869888
1945.057383	340054.226832	37.874906
1947.444041	340682.557865	37.879924
1949.310390	341334.292950	37.884941
1951.431189	341981.637137	37.889959
1953.153782	342646.678544	37.894976
1955.039381	343288.282639	37.899994
1957.015295	343944.888628	37.905012
1958.821856	344600.244541	37.910029
1961.194595	345272.299444	37.915047
1962.851252	345935.833921	37.920064
1964.618594	346599.670624	37.925082
1967.261081	347258.988155	37.930100
1968.735108	347926.737172	37.935117
1971.027670	348588.529681	37.940135
1972.928565	349267.837084	37.945152
1975.313546	349925.204385	37.950170
1976.877902	350593.228952	37.955188
1978.773575	351269.943676	37.960205
1981.157564	351935.833226	37.965223
1982.931067	352617.343424	37.970240
1985.012781	353283.236888	37.975258
1987.106716	353945.261028	37.980276
1988.830257	354623.220596	37.985293
1991.060394	355295.960099	37.990311
1993.212534	355966.950949	37.995328
1994.915333	356630.748433	38.000346
1996.871329	357307.281514	38.005364
1998.877225	357996.836780	38.010381
2001.070005	358666.813030	38.015399
2002.685894	359348.113187	38.020416
2004.671841	360026.346957	38.025434
2006.733570	360695.448617	38.030452
2008.706525	361354.151823	38.035469
2010.674504	362008.303669	38.040487
2012.709602	362665.807734	38.045504
2014.560485	363323.559492	38.050522
2016.658002	363972.836979	38.055540
2018.491714	364642.137368	38.060557
2020.779807	365301.609807	38.065575
2022.262665	365971.959596	38.070592
2024.018454	366640.654362	38.075610
2026.253139	367316.234005	38.080628
2027.903010	368002.982994	38.085645
2030.329828	368676.984335	38.090663
2032.135010	369373.853929	38.095680
2033.680000	370062.154650	38.100698
2035.868268	370753.354544	38.105716
2037.709393	371462.556085	38.110733
2039.870429	372163.625377	38.115751
2041.915431	372870.888614	38.120768
2043.765997	373581.492359	38.125786
2045.952065	374293.674965	38.130804
2047.889018	375019.122806	38.135821
2050.237043	375731.046602	38.140839
2052.388620	376459.801994	38.145856
2054.163639	377181.173823	38.150874
2056.201191	377905.530237	38.155892
2058.430588	378641.048051	38.160909
2060.635375	379367.932274	38.165927
2062.582653	380100.396598	38.170944
2064.514685	380842.051950	38.175962
2066.724090	381578.801945	38.180980
2068.966808	382319.916570	38.185997
2071.170218	383063.125459	38.191015
2073.218573	383800.181895	38.196032
2075.500791	384557.542235	38.201050
2077.430733	385286.902151	38.206068
2079.275071	386047.139327	38.211085
2081.722784	386793.061573	38.216103
2083.579016	387537.111855	38.221120
2085.926328	388293.561554	38.226138
2088.139440	389050.243313	38.231156
2090.579819	389810.240705	38.236173
2092.277210	390548.744658	38.241191
2094.796709	391301.949436	38.246208
2096.933154	392055.934022	38.251226
2099.031269	392796.396184	38.256244
2101.087644	393556.541483	38.261261
2103.571534	394310.463297	38.266279
2105.765355	395061.423267	38.271296
2107.680617	395807.822896	38.276314
2110.014291	396559.431564	38.281332
2112.111385	397310.654618	38.286349
2114.149974	398066.607169	38.291367
2116.326478	398808.300414	38.296384
2118.398009	399560.610087	38.301402
2120.651085	400309.550514	38.306420
2122.665869	401069.989800	38.311437
2124.852981	401822.550471	38.316455
2126.982716	402565.902666	38.321472
2129.121359	403332.291502	38.326490
2131.470022	404082.940878	38.331508
2133.680252	404837.672140	38.336525
2135.628194	405577.680602	38.341543
2138.097444	406332.733757	38.346560
2140.093128	407081.789355	38.351578
2142.243101	407826.998874	38.356596
2144.304960	408588.086505	38.361613
2146.764702	409338.270054	38.366631
2149.028633	410076.863030	38.371648
2150.997457	410793.674206	38.376666
2153.297682	411514.362980	38.381684
2155.163111	412234.242744	38.386701
2156.972799	412946.437367	38.391719
2159.310040	413662.628836	38.396736
2161.156051	414390.355265	38.401754
2163.406247	415124.402393	38.406772
2165.486729	415853.695404	38.411789
2167.724323	416589.678482	38.416807
2169.928944	417320.783536	38.421824
2172.054314	418055.451467	38.426842
2174.258385	418799.049683	38.431860
2175.759526	419548.870174	38.436877
2178.091709	420295.289990	38.441895
2180.364808	421047.976992	38.446912
2182.309914	421806.974895	38.451930
2184.506961	422574.491375	38.456948
2186.317843	423341.009708	38.461965
2188.427581	424118.037774	38.466983
2190.734707	424883.160166	38.472000
2192.543157	425669.252206	38.477018
2195.120286	426453.571717	38.482036
2197.007733	427240.865471	38.487053
2199.556689	428035.871571	38.492071
2201.783856	428835.410087	38.497088
2203.666960	429634.371050	38.502106
2206.124053	430423.743894	38.507124
2208.469584	431237.356189	38.512141
2210.453527	432049.228290	38.517159
2212.641668	432858.052047	38.522176
2214.770017	433672.172185	38.527194
2217.278041	434480.481646	38.532212
2219.461091	435310.124074	38.537229
2221.699371	436121.153391	38.542247
2223.947215	436946.019023	38.547264
2225.935075	437772.213376	38.552282
2228.191938	438586.845850	38.557300
2230.678408	439424.182248	38.562317
2232.985634	440254.786981	38.567335
2235.577081	441075.194022	38.572352
2237.413366	441910.368565	38.577370
2240.077111	442738.241015	38.582388
2242.067004	443579.448973	38.587405
2244.256239	444410.169851	38.592423
2246.852470	445246.862618	38.597440
2248.929658	446082.951117	38.602458
2251.121534	446912.361584	38.607476
2253.642259	447766.825831	38.612493
2255.911240	448595.450275	38.617511
2258.245469	449431.820970	38.622528
2260.597175	450277.158599	38.627546
2262.888430	451111.649155	38.632564
2265.139782	451955.772705	38.637581
2267.131668	452802.838156	38.642599
2269.558598	453642.464771	38.647616
2271.724423	454496.158215	38.652634
2274.201403	455339.095706	38.657652
2276.565196	456186.618548	38.662669
2278.493244	457027.453552	38.667687
2281.027444	457874.220900	38.672704
2283.145759	458726.127775	38.677722
2285.773601	459575.285767	38.682740
2288.278852	460415.075871	38.687757
2290.470669	461271.665250	38.692775
2292.992003	462118.660342	38.697792
2294.874862	462962.843516	38.702810
2297.235030	463802.565074	38.707828
2299.480561	464631.504286	38.712845
2301.659444	465459.358100	38.717863
2304.182954	466270.594107	38.722880
2306.014274	467092.624028	38.727898
2308.571489	467910.860853	38.732916
2310.756869	468733.318412	38.737933
2312.882778	469563.279400	38.742951
2315.231745	470381.142167	38.747968
2317.183982	471212.626444	38.752986
2319.987653	472047.369312	38.758004
2322.245715	472881.710663	38.763021
2324.555603	473724.948165	38.768039
2327.068099	474562.860674	38.773056
2328.978863	475411.897322	38.778074
2331.140172	476250.852670	38.783092
2333.319736	477095.424004	38.788109
2335.846302	477962.879865	38.793127
2338.288957	478809.652454	38.798144
2340.335869	479678.974950	38.803162
2342.641153	480543.769421	38.808180
2345.246652	481410.644530	38.813197
2347.423408	482290.727885	38.818215
2349.776743	483158.570534	38.823232
2352.193120	484048.323739	38.828250
2354.290387	484928.442279	38.833268
2356.600990	485808.936453	38.838285
2358.782286	486705.411006	38.843303
2361.717408	487595.860037	38.848320
2363.677855	488495.763008	38.853338
2366.188276	489394.115709	38.858356
2368.536184	490296.839981	38.863373
2370.836812	491196.497007	38.868391
2373.348011	492102.784529	38.873408
2375.918524	493021.378192	38.878426
2378.399656	493929.239718	38.883444
2380.749548	494835.863686	38.888461
2383.079429	495752.180606	38.893479
2385.576785	496673.919741	38.898496
2388.196082	497591.502000	38.903514
2390.469285	498501.423327	38.908532
2393.143110	499417.635607	38.913549
2395.170230	500352.012899	38.918567
2397.635415	501264.576660	38.923584
2400.714078	502186.874398	38.928602
2402.525683	503110.993931	38.933620
2405.305583	504033.035801	38.938637
2407.723673	504964.464964	38.943655
2410.224131	505881.859668	38.948672
2412.550886	506815.013266	38.953690
2414.993140	507739.724436	38.958708
2417.692329	508665.852635	38.963725
2420.098000	509594.395665	38.968743
2422.797586	510518.148135	38.973760
2424.871335	511446.940626	38.978778
2427.462635	512378.768848	38.983796
2429.706898	513301.476760	38.988813
2432.639626	514241.303682	38.993831
2434.831554	515165.573965	38.998848
2437.055861	516082.578145	39.003866
2439.772510	517016.377956	39.008884
2442.446907	517949.423127	39.013901
2444.343193	518877.502025	39.018919
2446.883816	519809.499499	39.023936
2449.482751	520741.380364	39.028954
2451.910235	521672.930462	39.033972
2454.293839	522603.826373	39.038989
2456.771779	523546.183879	39.044007
2459.403719	524463.879195	39.049024
2461.924975	525375.946702	39.054042
2464.226625	526288.146099	39.059060
2466.840484	527191.577173	39.064077
2469.315386	528084.402346	39.069095
2471.425099	528979.600538	39.074112
2473.970110	529877.240454	39.079130
2476.126423	530781.233159	39.084148
2479.083086	531687.806953	39.089165
2481.193291	532592.551469	39.094183
2483.882896	533493.469934	39.099200
2486.209296	534407.629591	39.104218
2488.367199	535321.356787	39.109236
2491.001675	536237.111538	39.114253
2492.847061	537173.217756	39.119271
2495.455118	538094.846744	39.124288
2497.993648	539031.773827	39.129306
2499.752365	539974.453158	39.134324
2503.000401	540922.911495	39.139341
2505.248155	541886.562684	39.144359
2507.758814	542841.754628	39.149376
2510.117250	543799.824018	39.154394
2512.267647	544781.249050	39.159412
2515.221721	545743.512815	39.164429
2517.407001	546722.230463	39.169447
2520.083136	547697.177554	39.174464
2522.429376	548684.127161	39.179482
2524.823664	549684.120193	39.184500
2527.755554	550678.019371	39.189517
2530.362259	551667.224807	39.194535
2533.193794	552662.855752	39.199552
2535.944288	553662.900247	39.204570
2538.345155	554665.793097	39.209588
2541.279100	555647.667735	39.214605
2543.660002	556663.330167	39.219623
2546.002529	557653.044654	39.224640
2549.031794	558653.274096	39.229658
2551.058243	559658.316079	39.234676
2554.143312	560653.009740	39.239693
2556.473030	561672.316205	39.244711
2559.155185	562682.645354	39.249728
2562.118848	563685.467163	39.254746
2564.623708	564694.113066	39.259764
2567.454413	565701.572405	39.264781
2570.171027	566715.901477	39.269799
2572.776876	567725.901411	39.274816
2575.375824	568735.270931	39.279834
2577.800269	569746.698171	39.284852
2580.770608	570754.642327	39.289869
2583.111974	571762.108507	39.294887
2585.652934	572769.010076	39.299904
2588.355338	573782.328802	39.304922
2590.743230	574792.707468	39.309940
2593.614964	575797.355475	39.314957
2596.231158	576820.127338	39.319975
2598.750846	577836.359583	39.324992
2601.283927	578845.333102	39.330010
2603.868055	579869.013213	39.335028
2607.067473	580884.281434	39.340045
2609.152100	581903.110240	39.345063
2611.776032	582917.904129	39.350080
2614.862750	583938.253778	39.355098
2617.064450	584958.363127	39.360116
2619.689279	585976.913232	39.365133
2622.179808	586995.800828	39.370151
2625.016048	588016.299778	39.375168
2627.614846	589043.618008	39.380186
2629.939738	590076.306082	39.385204
2632.879338	591081.040635	39.390221
2635.269184	592106.325869	39.395239
2638.175220	593102.827477	39.400256
2640.528671	594085.107662	39.405274
2643.031294	595070.938486	39.410292
2645.413007	596067.877195	39.415309
2647.954860	597066.658124	39.420327
2650.354575	598052.505564	39.425344
2653.148097	599049.622750	39.430362
2655.306479	600073.449144	39.435380
2657.616825	601085.593569	39.440397
2660.255465	602110.462101	39.445415
2662.758599	603135.662140	39.450432
2665.520890	604169.187438	39.455450
2667.872032	605214.099096	39.460468
2670.489598	606256.818981	39.465485
2673.154702	607311.345617	39.470503
2675.478583	608382.242990	39.475520
2678.024453	609441.344155	39.480538
2680.690387	610520.787729	39.485556
2683.356285	611610.582426	39.490573
2685.474840	612692.207885	39.495591
2687.956888	613801.676486	39.500608
2691.249536	614899.748324	39.505626
2693.715926	616012.548725	39.510644
2696.649183	617120.559820	39.515661
2699.158870	618245.377120	39.520679
2701.849587	619363.650375	39.525696
2704.893817	620490.148045	39.530714
2706.911158	621618.147763	39.535732
2709.998155	622739.507027	39.540749
2712.405582	623896.389517	39.545767
2715.211384	625039.242237	39.550784
2718.403313	626180.660592	39.555802
2720.857377	627348.653426	39.560820
2723.346314	628490.789881	39.565837
2726.627048	629650.302279	39.570855
2729.197475	630817.594801	39.575872
2731.879499	631990.581617	39.580890
2734.425832	633168.302650	39.585908
2737.541511	634326.828119	39.590925
2739.995551	635505.848675	39.595943
2743.060139	636693.219142	39.600960
2745.809739	637857.650398	39.605978
2748.344633	639043.441437	39.610996
2751.386094	640220.630802	39.616013
2754.078251	641407.719820	39.621031
2756.960139	642601.772580	39.626048
2760.208621	643775.526084	39.631066
2762.373555	644968.322317	39.636084
2765.483687	646147.359572	39.641101
2768.480346	647339.589394	39.646119
2770.948098	648535.952589	39.651136
2773.790136	649715.463447	39.656154
2776.514329	650907.962014	39.661172
2779.365533	652112.854619	39.666189
2782.116375	653304.563140	39.671207
2784.833351	654499.372071	39.676224
2788.189738	655691.838657	39.681242
2791.018087	656887.036932	39.686260
2793.863390	658073.022693	39.691277
2796.529832	659266.662120	39.696295
2799.175220	660467.975685	39.701312
2801.862703	661652.456099	39.706330
2805.305401	662861.257020	39.711348
2807.697048	664057.388035	39.716365
2810.580390	665245.525761	39.721383
2813.514580	666448.335880	39.726400
2816.657131	667621.904586	39.731418
2819.249226	668814.820495	39.736436
2821.985076	669967.571520	39.741453
2824.770660	671119.328372	39.746471
2827.432266	672270.766074	39.751488
2830.073148	673416.397835	39.756506
2833.131087	674574.647532	39.761524
2835.822546	675722.325278	39.766541
2838.823111	676882.584516	39.771559
2841.386087	678045.603696	39.776576
2843.923859	679201.325394	39.781594
2846.698651	680369.234872	39.786612
2849.580065	681554.415731	39.791629
2852.834632	682729.795195	39.796647
2854.935723	683919.219524	39.801664
2858.131900	685101.703443	39.806682
2860.869938	686297.415987	39.811700
2863.552096	687484.142924	39.816717
2866.494947	688688.441961	39.821735
2868.839444	689894.366111	39.826752
2871.809380	691108.759369	39.831770
2874.612913	692332.889529	39.836788
2877.690040	693556.707370	39.841805
2880.378555	694779.478345	39.846823
2882.992440	696015.980662	39.851840
2886.473153	697258.366030	39.856858
2889.297281	698502.915733	39.861876
2891.744027	699739.567553	39.866893
2895.496042	700990.948568	39.871911
2898.111626	702251.506739	39.876928
2901.186387	703499.120083	39.881946
2903.862853	704758.808713	39.886964
2907.099717	706009.749679	39.891981
2910.146320	707264.354577	39.896999
2912.975044	708539.465141	39.902016
2915.997140	709789.890960	39.907034
2919.003757	711055.287111	39.912052
2921.934663	712327.933388	39.917069
2925.172930	713591.428384	39.922087
2928.120604	714869.728659	39.927104
2931.233866	716130.587631	39.932122
2934.230204	717399.638078	39.937140
2937.133790	718678.058917	39.942157
2940.340992	719927.893011	39.947175
2943.141042	721210.542425	39.952192
2946.298405	722473.650934	39.957210
2949.351788	723747.558966	39.962228
2951.833040	725026.208729	39.967245
2955.308859	726289.322938	39.972263
2958.208880	727575.710705	39.977280
2961.122895	728841.488486	39.982298
2963.992261	730123.576399	39.987316
2966.929613	731394.140011	39.992333
2970.121353	732662.585709	39.997351
2972.770814	733953.733254	40.002368
2976.289559	735235.644067	40.007386
2979.030865	736507.309959	40.012404
2981.608413	737791.829725	40.017421
2984.558333	739082.644006	40.022439
2987.725928	740369.709914	40.027456
2990.718539	741659.703328	40.032474
2993.694082	742946.776321	40.037492
2996.456635	744237.520481	40.042509
2999.695498	745529.255888	40.047527
3002.553510	746830.453660	40.052544
3005.639660	748125.235949	40.057562
3008.474295	749415.803339	40.062580
3011.580001	750721.286928	40.067597
3014.822181	752018.350020	40.072615
3017.549492	753302.522835	40.077632
3020.607779	754550.969018	40.082650
3023.631046	755813.299916	40.087668
3026.521948	757066.681124	40.092685
3029.607329	758315.984798	40.097703
3032.186906	759569.103620	40.102720
3035.092300	760819.353589	40.107738
3037.834339	762086.150940	40.112756
3040.720977	763351.875234	40.117773
3043.751111	764633.149824	40.122791
3046.869470	765920.681507	40.127808
3049.480559	767195.980393	40.132826
3052.609658	768501.894551	40.137844
3055.249451	769800.484175	40.142861
3058.351026	771100.096632	40.147879
3061.162030	772421.734819	40.152896
3064.094277	773751.417094	40.157914
3067.133139	775075.585834	40.162932
3069.475807	776417.699536	40.167949
3073.000606	777765.115406	40.172967
3075.992121	779125.475071	40.177984
3079.212651	780478.425748	40.183002
3082.050872	781840.803130	40.188020
3084.826143	783212.254099	40.193037
3088.210569	784592.563738	40.198055
3091.209934	785986.450422	40.203072
3093.958520	787373.977742	40.208090
3097.335544	788773.042520	40.213108
3100.084625	790177.423902	40.218125
3103.833768	791581.998592	40.223143
3106.755928	792986.086829	40.228160
3109.767434	794400.802332	40.233178
3113.050710	795824.148869	40.238196
3116.369070	797238.827490	40.243213
3119.503142	798652.612736	40.248231
3122.551601	800080.561390	40.253248
3125.710285	801498.411333	40.258266
3129.187731	802949.769599	40.263284
3132.163339	804386.280487	40.268301
3135.460892	805801.606411	40.273319
3138.602996	807238.762591	40.278336
3141.603380	808680.673480	40.283354
3145.476980	810112.116438	40.288372
3148.379905	811554.409715	40.293389
3151.553677	812988.632370	40.298407
3155.185811	814430.678396	40.303424
3157.819179	815864.278602	40.308442
3161.183892	817301.453919	40.313460
3164.388213	818749.229454	40.318477
3167.867817	820192.350379	40.323495
3170.676393	821640.146009	40.328512
3174.272841	823091.298837	40.333530
3177.785121	824530.198984	40.338548
3180.653800	825979.127727	40.343565
3184.106295	827423.399099	40.348583
3187.203228	828867.896726	40.353600
3190.115512	830318.242713	40.358618
3193.641527	831768.893894	40.363636
3196.476346	833217.872622	40.368653
3199.832410	834669.799163	40.373671
3202.737184	836153.792466	40.378688
3206.210121	837618.126193	40.383706
3209.493654	839080.549887	40.388724
3212.447201	840559.619409	40.393741
3215.805419	842010.266615	40.398759
3219.066699	843488.601947	40.403776
3221.975937	844960.718816	40.408794
3225.088878	846440.038668	40.413812
3228.334655	847922.097125	40.418829
3231.704504	849361.330694	40.423847
3234.917927	850797.732501	40.428864
3237.950705	852239.366937	40.433882
3241.140869	853681.999179	40.438900
3244.552212	855127.849228	40.443917
3247.848099	856570.564949	40.448935
3251.123619	858027.690814	40.453952
3254.061924	859487.241185	40.458970
3257.469444	860946.268371	40.463988
3260.546228	862422.934457	40.469005
3263.565892	863882.193189	40.474023
3266.760414	865365.779198	40.479040
3269.520042	866857.596594	40.484058
3273.287462	868370.474516	40.489076
3276.352457	869884.829223	40.494093
3279.174492	871392.064600	40.499111
3282.647167	872915.456373	40.504128
3286.118982	874454.614388	40.509146
3289.559197	875994.635007	40.514164
3292.349459	877543.353805	40.519181
3295.740746	879113.220311	40.524199
3298.990081	880668.966684	40.529216
3302.060289	882247.710537	40.534234
3305.626887	883828.263392	40.539252
3308.898107	885414.711913	40.544269
3312.538218	887009.450374	40.549287
3315.956605	888609.093230	40.554304
3318.942771	890208.169902	40.559322
3322.230240	891798.552428	40.564340
3325.555498	893421.948455	40.569357
3329.364074	895052.129423	40.574375
3332.796429	896662.918712	40.579392
3336.009046	898299.300497	40.584410
3339.453109	899912.823626	40.589428
3342.940740	901566.898013	40.594445
3346.582133	903191.868958	40.599463
3350.149362	904815.802647	40.604480
3353.410316	906457.785906	40.609498
3357.331212	908082.824749	40.614516
3360.735978	909718.433288	40.619533
3364.277256	911368.337919	40.624551
3367.897267	913002.936551	40.629568
3371.057247	914636.259468	40.634586
3375.348844	916259.016420	40.639604
3378.231949	917907.252707	40.644621
3381.939468	919538.153010	40.649639
3385.485304	921165.518602	40.654656
3388.838974	922798.084889	40.659674
3392.602089	924430.855829	40.664692
3395.861111	926067.814505	40.669709
3399.917077	927682.674243	40.674727
3403.436685	929317.060757	40.679744
3406.446968	930936.470912	40.684762
3410.169517	932547.226271	40.689780
3413.708149	934199.157630	40.694797
3417.434720	935821.738263	40.699815
3420.792536	937428.573027	40.704832
3424.214504	939052.308255	40.709850
3427.853337	940655.618082	40.714868
3431.247980	942277.109878	40.719885
3434.870725	943892.420342	40.724903
3438.474709	945507.993280	40.729920
3441.523676	947122.291944	40.734938
3445.050437	948726.555336	40.739956
3448.629439	950331.929838	40.744973
3452.231955	951941.565272	40.749991
3455.812635	953575.005964	40.755008
3458.990990	955200.270683	40.760013
3462.597440	956776.131494	40.765018
3465.858920	958302.806243	40.770023
3469.204009	959757.136853	40.775028
3472.493402	961139.592554	40.780032
3475.117763	962451.304662	40.785037
3478.739458	963692.635034	40.790042
3481.579926	964849.529798	40.795047
3484.301533	965933.872960	40.800052
3487.409316	966930.843856	40.805056
3489.603643	967867.611955	40.810061
3492.573374	968724.849759	40.815066
3495.046350	969507.008902	40.820071
3497.186461	970218.494718	40.825076
3499.321673	970862.017954	40.830080
3501.464659	971451.681616	40.835085
3503.641140	971948.188757	40.840090
3505.341636	972388.998522	40.845095
3507.167499	972779.011008	40.850100
3509.046710	973107.494324	40.855104
3510.542408	973391.345779	40.860109
3512.494070	973604.235068	40.865114
3514.095590	973783.644804	40.870119
3515.258437	973900.071896	40.875124
3516.629489	973967.880676	40.880128
3517.734488	974012.272663	40.885133
3519.203099	973990.428171	40.890138
3520.136190	973955.964285	40.895143
3521.109291	973860.887680	40.900148
3522.649814	973750.368686	40.905152
3523.131712	973597.400293	40.910157
3523.993943	973411.322488	40.915162
3524.748816	973208.929914	40.920167
3525.308123	972968.726625	40.925172
3526.159966	972710.866213	40.930176
3526.608308	972427.149975	40.935181
3527.489130	972110.689400	40.940186
3528.065457	971787.220839	40.945191
3528.288505	971444.429203	40.950196
3528.958371	971079.832026	40.955200
3529.987950	970699.992518	40.960205
3530.426216	970314.943409	40.965210
3530.890643	969883.399908	40.970215
3531.179609	969461.635567	40.975220
3531.602725	969006.456556	40.980224
3531.784036	968552.161865	40.985229
3532.137698	968079.406942	40.990234
3532.526911	967601.127151	40.995239
3532.530684	967111.420587	41.000244
3532.883307	966614.763511	41.005248
3532.820636	966107.168898	41.010253
3533.216191	965600.334986	41.015258
3533.307981	965083.422569	41.020263
3533.497395	964556.754446	41.025268
3533.629684	964021.920165	41.030272
3533.536221	963494.026281	41.035277
3534.049156	962954.035642	41.040282
3534.200725	962396.521319	41.045287
3534.252363	961844.748908	41.050292
3534.419246	961279.385281	41.055296
3534.135822	960721.192577	41.060301
3534.404730	960152.468316	41.065306
3534.449118	959580.981042	41.070311
3534.602847	959014.319329	41.075316
3535.099660	958431.470988	41.080320
3534.781177	957859.774837	41.085325
3534.971376	957263.331556	41.090330
3535.100128	956676.052940	41.095335
3534.977504	956084.245455	41.100340
3535.447486	955483.257696	41.105344
3534.935683	954891.588185	41.110349
3534.978505	954283.288366	41.115354
3535.227741	953686.563852	41.120359
3535.282509	953073.229899	41.125364
3535.135019	952477.628443	41.130368
3535.092941	951882.350108	41.135373
3535.275719	951293.564653	41.140378
3534.985331	950707.084908	41.145383
3535.264900	950110.781523	41.150388
3535.316866	949512.149790	41.155392
3534.884159	948911.709765	41.160397
3535.148517	948302.854243	41.165402
3534.904314	947708.462734	41.170407
3534.753914	947115.327065	41.175412
3534.763862	946510.799909	41.180416
3534.490370	945922.908096	41.185421
3534.572653	945322.442276	41.190426
3534.730099	944725.341788	41.195431
3534.366935	944128.641133	41.200436
3534.283860	943522.342279	41.205440
3534.223414	942935.320391	41.210445
3534.179600	942332.899414	41.215450
3534.366777	941746.276960	41.220455
3534.023066	941145.588195	41.225460
3534.250343	940551.445058	41.230464
3534.300965	939953.237277	41.235469
3534.299061	939348.067082	41.240474
3534.091967	938753.982285	41.245479
3533.928485	938155.220069	41.250484
3534.047605	937547.615862	41.255488
3533.681026	936965.916982	41.260493
3533.902069	936363.913281	41.265498
3533.557879	935759.727185	41.270503
3533.308968	935170.231137	41.275508
3533.400519	934573.704224	41.280512
3533.133478	933986.861234	41.285517
3532.929248	933396.295479	41.290522
3532.657476	932803.563049	41.295527
3533.008519	932230.916808	41.300532
3532.759963	931633.057459	41.305536
3532.445356	931057.225620	41.310541
3532.399083	930476.197502	41.315546
3532.511051	929894.791572	41.320551
3532.195636	929309.742541	41.325556
3532.058117	928728.826467	41.330560
3531.963272	928155.429531	41.335565
3532.207233	927579.128749	41.340570
3532.164864	927009.827544	41.345575
3531.548484	926433.064332	41.350580
3531.363967	925861.646106	41.355584
3531.312871	925294.470381	41.360589
3531.459624	924727.971092	41.365594
3531.454329	924146.919577	41.370599
3530.989391	923598.380435	41.375604
3530.867151	923024.053571	41.380608
3530.732101	922472.075709	41.385613
3530.926970	921905.174893	41.390618
3530.719326	921343.667595	41.395623
3530.218651	920796.388109	41.400628
3530.557674	920234.771715	41.405632
3530.198555	919679.081610	41.410637
3529.778774	919126.808837	41.415642
3530.216727	918572.702402	41.420647
3529.709224	918032.844126	41.425652
3529.859928	917479.636048	41.430656
3529.602541	916941.264628	41.435661
3529.783925	916389.577333	41.440666
3529.385372	915852.180657	41.445671
3529.047084	915307.402393	41.450676
3529.197386	914770.482941	41.455680
3528.876560	914243.990760	41.460685
3528.627789	913710.211526	41.465690
3528.455537	913182.629583	41.470695
3528.581815	912643.578896	41.475700
3528.433365	912123.695293	41.480704
3528.387874	911599.987357	41.485709
3528.274346	911074.216950	41.490714
3528.214017	910537.399954	41.495719
3528.032488	910025.516237	41.500724
3528.068161	909498.028711	41.505728
3528.064168	908981.006090	41.510733
3527.981158	908467.129997	41.515738
3527.860385	907952.344585	41.520743
3527.337696	907441.435056	41.525748
3527.383383	906919.679337	41.530752
3526.925910	906411.847012	41.535757
3527.006695	905907.448767	41.540762
3526.973027	905395.884713	41.545767
3526.669999	904894.062660	41.550772
3526.866420	904397.323604	41.555776
3526.517179	903902.174218	41.560781
3526.387171	903395.846534	41.565786
3526.355528	902918.121898	41.570791
3526.213967	902423.096880	41.575796
3526.213588	901920.861475	41.580800
3525.701365	901439.518254	41.585805
3525.997357	900956.166170	41.590810
3525.540864	900467.778957	41.595815
3525.098222	899993.349064	41.600820
3525.386331	899524.553210	41.605824
3525.190884	899043.918489	41.610829
3525.462747	898570.023709	41.615834
3525.344541	898096.443222	41.620839
3525.175187	897617.421532	41.625844
3524.978449	897138.750246	41.630848
3524.853120	896669.109233	41.635853
3524.800930	896187.918229	41.640858
3524.372689	895731.197912	41.645863
3524.202321	895270.049288	41.650868
3524.174796	894809.612942	41.655872
3523.923947	894357.102383	41.660877
3523.807968	893893.223309	41.665882
3523.552258	893453.305442	41.670887
3523.718088	893001.295306	41.675892
3523.912793	892555.819704	41.680896
3523.592452	892108.363536	41.685901
3523.474775	891665.674328	41.690906
3523.463135	891214.809368	41.695911
3522.971102	890773.466868	41.700916
3523.131262	890324.824932	41.705920
3522.791639	889894.513617	41.710925
3522.401638	889454.987636	41.715930
3522.637476	889022.291072	41.720935
3522.450498	888592.534409	41.725940
3522.571760	888154.179454	41.730944
3522.164725	887739.490950	41.735949
3522.289702	887302.038343	41.740954
3521.958183	886886.889006	41.745959
3521.958611	886460.523760	41.750964
3521.903663	886035.781839	41.755968
3521.590728	885615.988512	41.760973
3521.488970	885199.808972	41.765978
3521.828924	884783.720431	41.770983
3521.039780	884367.788085	41.775988
3521.186656	883967.359243	41.780992
3521.068228	883567.624430	41.785997
3521.170576	883156.300646	41.791002
3521.193017	882766.463129	41.796007
3520.802294	882355.164002	41.801012
3520.807851	881953.360697	41.806016
3520.444045	881559.728208	41.811021
3520.394393	881159.623146	41.816026
3520.435937	880770.230418	41.821031
3520.404893	880381.114420	41.826036
3520.452733	879996.223266	41.831040
3520.375777	879601.248877	41.836045
3519.890785	879200.887843	41.841050
3520.070775	878820.161998	41.846055
3519.597544	878428.760073	41.851060
3519.727874	878051.772817	41.856064
3519.488327	877667.745670	41.861069
3519.359902	877287.746932	41.866074
3519.262716	876926.042671	41.871079
3518.981809	876553.099241	41.876084
3519.202891	876173.455888	41.881088
3519.191518	875816.905611	41.886093
3519.031057	875445.617855	41.891098
3518.963988	875076.812961	41.896103
3518.360410	874720.003149	41.901108
3518.536546	874352.955877	41.906112
3518.466896	874007.654592	41.911117
3517.960254	873656.778817	41.916122
3518.076279	873295.593399	41.921127
3517.885898	872946.466763	41.926132
3517.808900	872599.241410	41.931136
3517.702727	872264.226292	41.936141
3518.061334	871911.940562	41.941146
3517.872317	871558.462691	41.946151
3517.249763	871223.571140	41.951156
3517.173085	870874.886531	41.956160
3517.113324	870545.299074	41.961165
3517.352677	870218.944275	41.966170
3517.372725	869882.706856	41.971175
3517.117560	869546.204653	41.976180
3517.314518	869209.317796	41.981184
3517.048771	868890.157560	41.986189
3517.029356	868555.599604	41.991194
3516.959763	868224.915045	41.996199
3517.126718	867904.757206	42.001204
3516.952066	867569.684348	42.006208
3516.912433	867248.457400	42.011213
3516.295791	866910.507281	42.016218
3516.721387	866600.046047	42.021223
3516.129569	866283.908859	42.026228
3516.414591	865957.897461	42.031232
3516.297675	865660.395663	42.036237
3515.887150	865339.905076	42.041242
3515.861319	865013.116695	42.046247
3515.771264	864711.483523	42.051252
3515.414529	864400.260736	42.056256
3515.651406	864105.733055	42.061261
3515.782697	863803.046483	42.066266
3515.295383	863500.641039	42.071271
3515.151600	863212.837432	42.076276
3515.594757	862899.267815	42.081280
3515.298166	862608.253723	42.086285
3515.181541	862307.379824	42.091290
3515.362453	862008.191504	42.096295
3514.950994	861718.514416	42.101300
3515.149743	861418.419333	42.106304
3515.094138	861129.238769	42.111309
3515.193607	860847.018293	42.116314
3515.186847	860556.635926	42.121319
3514.813411	860267.466808	42.126324
3514.990080	859972.748604	42.131328
3514.629406	859689.383613	42.136333
3514.268330	859400.754760	42.141338
3514.224703	859114.977196	42.146343
3513.949726	858842.158041	42.151348
3514.149705	858554.563728	42.156352
3514.157951	858282.256437	42.161357
3513.803606	858008.246119	42.166362
3514.045769	857736.070523	42.171367
3513.727634	857464.656026	42.176372
3514.131840	857196.709553	42.181376
3513.589272	856936.592154	42.186381
3513.271117	856669.130765	42.191386
3513.789490	856391.110491	42.196391
3512.915148	856134.516008	42.201396
3513.135645	855877.535841	42.206400
3513.342914	855629.498395	42.211405
3513.187391	855357.866718	42.216410
3513.254971	855109.928661	42.221415
3512.706315	854851.864759	42.226420
3512.893776	854596.296212	42.231424
3513.108747	854362.706083	42.236429
3513.124693	854108.118743	42.241434
3513.103536	853847.395582	42.246439
3512.954008	853594.760835	42.251444
3513.110829	853331.748042	42.256448
3512.724021	853085.068846	42.261453
3512.896420	852833.712681	42.266458
3512.713942	852594.767505	42.271463
3512.801952	852366.476809	42.276468
3512.454291	852099.990285	42.281472
3512.484021	851865.654923	42.286477
3512.116684	851622.126989	42.291482
3512.383427	851377.998210	42.296487
3512.180925	851133.158211	42.301492
3512.562369	850884.999111	42.306496
3512.377964	850669.543838	42.311501
3512.119126	850423.224539	42.316506
3511.977244	850183.498195	42.321511
3512.035871	849958.921738	42.326516
3512.048293	849720.125986	42.331520
3511.777427	849488.769617	42.336525
3511.930040	849256.945303	42.341530
3511.880494	849026.509282	42.346535
3511.425434	848802.949814	42.351540
3511.880110	848571.147662	42.356544
3511.366822	848355.179507	42.361549
3511.458452	848127.609366	42.366554
3511.816466	847898.623208	42.371559
3511.331182	847669.280504	42.376564
3511.189451	847451.856024	42.381568
3511.627241	847238.128202	42.386573
3511.348633	847023.731673	42.391578
3511.425506	846806.443634	42.396583
3511.459886	846575.513727	42.401588
3511.235394	846358.454693	42.406592
3511.158735	846143.312689	42.411597
3510.905630	845917.375614	42.416602
3510.999351	845704.919073	42.421607
3510.652810	845501.396288	42.426612
3510.470348	845292.479682	42.431616
3510.553324	845091.406766	42.436621
3510.357151	844877.800501	42.441626
3510.777080	844674.806934	42.446631
3510.150539	844482.895966	42.451636
3510.561133	844276.089732	42.456640
3510.399948	844081.945450	42.461645
3510.148546	843867.144284	42.466650
3510.301795	843671.570837	42.471655
3510.114652	843482.481501	42.476660
3510.084809	843284.879029	42.481664
3510.312552	843100.486864	42.486669
3510.060781	842898.326735	42.491674
3510.070128	842694.557143	42.496679
3509.870670	842516.945719	42.501684
3509.962353	842303.009828	42.506688
3509.532265	842121.622630	42.511693
3509.738970	841938.418890	42.516698
3509.909105	841741.417804	42.521703
3509.797760	841573.614192	42.526708
3509.810924	841371.897975	42.531712
3509.909682	841182.497730	42.536717
3509.398732	840983.586114	42.541722
3509.451419	840798.375549	42.546727
3509.226340	840629.883009	42.551732
3509.589548	840436.759559	42.556736
3509.337808	840255.777245	42.561741
3509.511744	840077.499489	42.566746
3509.026886	839900.105608	42.571751
3509.147597	839726.411216	42.576756
3509.287473	839551.099407	42.581760
3509.216034	839379.963430	42.586765
3509.072309	839193.323995	42.591770
3508.798694	839012.846450	42.596775
3508.816141	838850.998096	42.601780
3509.061707	838677.791097	42.606784
3508.792775	838513.396015	42.611789
3508.857960	838339.282698	42.616794
3508.965203	838162.816073	42.621799
3508.717536	837997.867577	42.626804
3508.891093	837837.138624	42.631808
3508.379606	837677.250309	42.636813
3509.034031	837502.187695	42.641818
3508.711855	837328.696113	42.646823
3508.407903	837174.274319	42.651828
3508.603485	837009.227268	42.656832
3508.384166	836854.539845	42.661837
3508.024852	836697.822353	42.666842
3508.734988	836530.726382	42.671847
3508.493772	836360.903739	42.676852
3508.417459	836204.664324	42.681856
3508.424453	836049.188175	42.686861
3508.310800	835885.871129	42.691866
3508.285098	835719.216857	42.696871
3508.119356	835568.881791	42.701876
3508.170115	835409.771455	42.706880
3508.492606	835254.175253	42.711885
3508.004242	835112.472520	42.716890
3508.132135	834942.258653	42.721895
3507.706893	834792.729101	42.726900
3507.646667	834639.865608	42.731904
3507.821022	834499.797356	42.736909
3507.740051	834347.027944	42.741914
3508.044694	834206.394897	42.746919
3507.853958	834065.205801	42.751924
3507.701605	833905.359465	42.756928
3507.503835	833767.972682	42.761933
3507.504294	833621.421254	42.766938
3507.445195	833467.504540	42.771943
3507.408614	833329.740116	42.776948
3507.628479	833198.082033	42.781952
3507.559786	833065.882934	42.786957
3507.546361	832915.558400	42.791962
3507.440994	832763.194863	42.796967
3507.171517	832634.242450	42.801972
3507.503819	832483.362629	42.806977
3507.690595	832343.733752	42.811981
3507.524140	832208.847659	42.816986
3507.487385	832066.124544	42.821991
3507.383514	831929.122600	42.826996
3507.096602	831785.457877	42.832001
3507.186452	831654.278076	42.837005
3507.176900	831512.124252	42.842010
3507.413484	831385.163416	42.847015
3507.069133	831257.367916	42.852020
3507.156073	831109.377820	42.857025
3507.268534	830977.887565	42.862029
3507.244755	830839.335363	42.867034
3507.311102	830696.760422	42.872039
3506.727907	830570.797827	42.877044
3506.940027	830444.994801	42.882049
3506.985448	830329.229699	42.887053
3506.807480	830204.609680	42.892058
3506.760935	830071.173466	42.897063
3506.542771	829950.658197	42.902068
3506.727547	829812.098537	42.907073
3506.793041	829686.158424	42.912077
3506.644475	829563.670578	42.917082
3506.596500	829440.235698	42.922087
3506.580684	829323.241501	42.927092
3506.458689	829185.305235	42.932097
3506.623641	829074.822946	42.937101
3506.452398	828940.016169	42.942106
3506.510877	828820.460290	42.947111
3506.518392	828709.900036	42.952116
3506.300283	828592.242046	42.957121
3506.491796	828472.853291	42.962125
3506.368616	828357.276278	42.967130
3506.678157	828225.209261	42.972135
3506.302816	828114.017943	42.977140
3506.295124	827993.529449	42.982145
3506.394098	827879.861804	42.987149
3505.918132	827761.840406	42.992154
3505.933819	827647.058585	42.997159
3505.892069	827535.411526	43.002164
3505.973885	827428.482118	43.007169
3505.916418	827315.514528	43.012173
3505.916923	827203.170702	43.017178
3505.906800	827093.221209	43.022183
3505.911822	826980.237524	43.027188
3505.871830	826872.781535	43.032193
3505.823527	826768.452834	43.037197
3505.881457	826661.808034	43.042202
3505.800187	826563.688095	43.047207
3505.653276	826465.137646	43.052212
3505.937331	826352.097134	43.057217
3505.907111	826239.301946	43.062221
3505.988988	826126.730719	43.067226
3505.922803	826034.807467	43.072231
3505.812284	825932.039695	43.077236
3505.897215	825811.251314	43.082241
3505.634926	825716.472147	43.087245
3505.630563	825626.194823	43.092250
3505.515347	825509.001983	43.097255
3505.533803	825418.424760	43.102260
3505.445301	825305.476452	43.107265
3505.463522	825205.462287	43.112269
3505.136535	825099.686456	43.117274
3505.441103	824994.733646	43.122279
3505.155178	824912.265323	43.127284
3505.033570	824813.245896	43.132289
3505.631184	824722.905841	43.137293
3505.336792	824637.600112	43.142298
3505.589057	824540.079316	43.147303
3505.059127	824436.917232	43.152308
3505.273002	824342.724179	43.157313
3505.170762	824256.795184	43.162317
3505.415244	824150.176563	43.167322
3505.596193	824049.726867	43.172327
3505.079466	823957.897631	43.177332
3505.224744	823864.491287	43.182337
3505.387306	823775.578870	43.187341
3505.271831	823689.791322	43.192346
3505.283950	823589.557989	43.197351
3504.954310	823505.759077	43.202356
3505.505983	823400.153367	43.207361
3505.397415	823313.039601	43.212365
3505.045002	823216.087765	43.217370
3505.214075	823124.818453	43.222375
3505.140206	823032.463254	43.227380
3505.002709	822950.337039	43.232385
3505.174532	822858.819099	43.237389
3504.944425	822767.512811	43.242394
3505.449385	822665.766124	43.247399
3505.101117	822582.447537	43.252404
3505.031365	822487.443355	43.257409
3505.236976	822396.304646	43.262413
3505.172328	822307.605469	43.267418
3504.965018	822211.788626	43.272423
3504.682662	822126.203829	43.277428
3504.749799	822034.007032	43.282433
3504.628368	821942.231265	43.287437
3504.676757	821873.216706	43.292442
3504.990400	821790.414841	43.297447
3504.487645	821705.496694	43.302452
3504.405984	821619.725541	43.307457
3504.966786	821543.042307	43.312461
3504.839264	821454.293118	43.317466
3504.758371	821370.621718	43.322471
3504.572362	821294.107556	43.327476
3504.638034	821206.741625	43.332481
3504.679969	821127.595673	43.337485
3504.670514	821042.098602	43.342490
3504.972790	820964.766490	43.347495
3504.762963	820885.169987	43.352500
3504.562571	820801.070848	43.357505
3504.605031	820728.963716	43.362509
3504.443343	820653.465350	43.367514
3504.634856	820561.814522	43.372519
3504.460514	820491.452591	43.377524
3504.589045	820409.055279	43.382529
3504.827151	820330.699076	43.387533
3504.434162	820258.022631	43.392538
3504.537168	820165.011183	43.397543
3504.401696	820091.899133	43.402548
3504.240733	820013.017890	43.407553
3504.527785	819939.492102	43.412557
3504.398068	819866.474460	43.417562
3504.669895	819785.660196	43.422567
3504.603350	819711.260623	43.427572
3504.440457	819624.205018	43.432577
3504.490024	819550.469435	43.437581
3504.144647	819497.052689	43.442586
3504.451042	819405.318030	43.447591
3504.308890	819340.369220	43.452596
3504.460388	819259.079123	43.457601
3504.457633	819184.320653	43.462605
3504.513730	819106.567104	43.467610
3504.416915	819024.825784	43.472615
3504.183477	818959.790437	43.477620
3504.332838	818887.939249	43.482625
3504.378183	818805.584668	43.487629
3503.947937	818736.812020	43.492634
3504.408173	818669.849148	43.497639
3504.310321	818596.861224	43.502644
3503.973443	818526.652028	43.507649
3504.391803	818450.347985	43.512653
3503.649875	818393.904999	43.517658
3503.944220	818321.730215	43.522663
3503.764489	818253.009151	43.527668
3503.791284	818186.357498	43.532673
3504.044136	818121.233826	43.537677
3503.685008	818055.035917	43.542682
3503.976040	817989.513190	43.547687
3504.083529	817935.079500	43.552692
3504.081570	817857.810277	43.557697
3504.035424	817788.083682	43.562701
3504.062805	817725.440122	43.567706
3503.911316	817664.195695	43.572711
3504.158676	817594.663405	43.577716
3504.080572	817533.209932	43.582721
3503.858173	817456.021309	43.587725
3503.904255	817385.932737	43.592730
3503.980741	817322.004867	43.597735
3503.732257	817261.164238	43.602740
3504.141135	817192.041605	43.607745
3503.755818	817137.780484	43.612749
3503.735909	817066.818487	43.617754
3503.945656	817005.312722	43.622759
3503.792698	816952.822679	43.627764
3503.809429	816883.467806	43.632769
3504.187523	816820.513248	43.637773
3503.734112	816758.771869	43.642778
3504.219955	816695.113159	43.647783
3503.672552	816628.246870	43.652788
3503.617118	816557.578984	43.657793
3503.925890	816493.898587	43.662797
3503.583549	816431.646420	43.667802
3503.986843	816373.920785	43.672807
3503.829136	816312.958659	43.677812
3503.534216	816237.285257	43.682817
3503.827576	816183.247188	43.687821
3504.158879	816135.369974	43.692826
3504.086976	816058.972527	43.697831
3503.858701	816012.557212	43.702836
3503.579188	815936.388368	43.707841
3503.721613	815878.309838	43.712845
3503.547180	815823.758534	43.717850
3503.875574	815758.746230	43.722855
3503.815452	815709.217160	43.727860
3503.677246	815632.091482	43.732865
3503.719206	815574.124772	43.737869
3503.387097	815519.548013	43.742874
3503.932970	815451.755517	43.747879
3503.697955	815403.476842	43.752884
3503.768496	815338.111309	43.757889
3504.058929	815279.366790	43.762893
3503.806279	815213.416875	43.767898
3503.856126	815143.499992	43.772903
3503.628115	815089.832741	43.777908
3503.540096	815035.897211	43.782913
3503.716868	814978.001044	43.787917
3503.536129	814933.332868	43.792922
3503.460132	814863.140050	43.797927
3503.832752	814805.210124	43.802932
3503.632353	814742.674056	43.807937
3503.842673	814675.075876	43.812941
3503.407594	814628.978795	43.817946
3503.680234	814563.572412	43.822951
3503.382183	814513.535140	43.827956
3503.419496	814456.734586	43.832961
3503.476512	814399.783420	43.837965
3503.219797	814351.745548	43.842970
3503.373411	814289.440696	43.847975
3503.083227	814245.765216	43.852980
3503.414525	814190.382846	43.857985
3503.216706	814131.121167	43.862989
3502.818171	814091.673384	43.867994
3503.343797	814049.331120	43.872999
3503.513087	814004.403229	43.878004
3503.259832	813947.205560	43.883009
3503.372492	813890.485731	43.888013
3503.198104	813846.641679	43.893018
3503.717667	813789.658096	43.898023
3503.498121	813730.347494	43.903028
3503.530752	813680.641257	43.908033
3503.299658	813626.424170	43.913037
3503.031055	813577.795113	43.918042
3503.259694	813522.913835	43.923047
3503.560573	813482.612718	43.928052
3503.401021	813430.977575	43.933057
3503.730838	813369.026909	43.938061
3503.379761	813319.038438	43.943066
3503.327637	813250.538753	43.948071
3503.240543	813201.730159	43.953076
3503.326134	813152.403054	43.958081
3503.506513	813103.402766	43.963085
3503.248297	813057.314715	43.968090
3503.241826	813005.161370	43.973095
3503.027694	812950.054545	43.978100
3503.208191	812903.158575	43.983105
3503.606747	812862.396903	43.988109
3503.524977	812812.703104	43.993114
3503.286481	812740.653909	43.998119
3503.256915	812687.914229	44.003124
3503.190345	812644.240466	44.008129
3503.452844	812603.009902	44.013133
3503.343788	812554.836905	44.018138
3503.127784	812497.669741	44.023143
3503.182568	812452.260605	44.028148
3502.999637	812395.576881	44.033153
3503.140410	812338.692417	44.038157
3503.311988	812305.311236	44.043162
3503.729442	812258.763557	44.048167
3503.195626	812208.209215	44.053172
3503.395832	812150.382800	44.058177
3503.652540	812100.627981	44.063181
3503.059626	812054.098426	44.068186
3503.312101	811998.025319	44.073191
3503.364419	811956.678500	44.078196
3503.439266	811901.760382	44.083201
3503.647369	811852.207658	44.088205
3503.253384	811800.647619	44.093210
3503.186769	811737.130926	44.098215
3503.236525	811695.097196	44.103220
3503.130836	811642.802714	44.108225
3503.049284	811604.855516	44.113229
3503.131609	811551.010911	44.118234
3503.017226	811502.096538	44.123239
3502.926304	811460.721299	44.128244
3503.169851	811407.730679	44.133249
3503.305854	811361.664041	44.138253
3502.656852	811321.457536	44.143258
3502.891943	811266.262929	44.148263
3502.950296	811227.849704	44.153268
3502.978971	811185.767293	44.158273
3502.860648	811136.948893	44.163277
3502.629442	811115.874472	44.168282
3502.876217	811075.616881	44.173287
3502.865003	811032.609363	44.178292
3502.717284	810981.002483	44.183297
3502.712952	810944.214522	44.188301
3502.751052	810907.762276	44.193306
3502.832417	810866.795894	44.198311
3503.053988	810820.662486	44.203316
3502.463160	810784.362186	44.208321
3502.965213	810738.230990	44.213325
3502.921582	810707.130823	44.218330
3502.860594	810653.694590	44.223335
3502.824461	810622.004932	44.228340
3502.930982	810577.848379	44.233345
3503.028259	810536.926368	44.238349
3503.062834	810484.599812	44.243354
3503.181636	810441.420144	44.248359
3502.895802	810399.972545	44.253364
3502.497043	810351.733577	44.258369
3502.765268	810313.574526	44.263373
3502.549456	810272.114607	44.268378
3502.826456	810244.486865	44.273383
3503.016481	810211.876176	44.278388
3502.664380	810162.795311	44.283393
3503.113086	810124.703446	44.288397
3502.759378	810080.668473	44.293402
3502.769708	810048.429554	44.298407
3502.923920	810005.780197	44.303412
3502.950761	809960.603889	44.308417
3503.011622	809910.228311	44.313421
3502.697263	809874.465497	44.318426
3503.192156	809829.064212	44.323431
3503.040570	809788.864610	44.328436
3502.808559	809746.816204	44.333441
3502.930329	809695.547081	44.338445
3502.935161	809654.340999	44.343450
3503.003523	809624.589291	44.348455
3502.933344	809588.343769	44.353460
3502.951494	809538.707412	44.358465
3503.076129	809493.217897	44.363469
3502.632646	809450.075560	44.368474
3502.503697	809406.587138	44.373479
3502.808431	809370.229680	44.378484
3502.684008	809345.016318	44.383489
3502.964805	809291.072039	44.388493
3502.965945	809266.229684	44.393498
3503.071250	809208.246771	44.398503
3502.966577	809177.590631	44.403508
3503.022935	809135.343920	44.408513
3503.046080	809098.051410	44.413517
3503.037676	809053.070864	44.418522
3502.759675	809002.695378	44.423527
3503.022746	808961.246536	44.428532
3502.873638	808928.391552	44.433537
3503.137466	808881.551975	44.438541
3502.590955	808845.674975	44.443546
3502.746241	808797.480654	44.448551
3503.005383	808751.866007	44.453556
3502.727790	808724.372462	44.458561
3502.811471	808679.570281	44.463565
3502.729804	808656.160421	44.468570
3502.869455	808599.342725	44.473575
3502.710629	808572.074012	44.478580
3502.580256	808538.577006	44.483585
3502.937187	808497.550909	44.488589
3502.593713	808450.416389	44.493594
3502.781260	808426.128302	44.498599
3502.698385	808390.515537	44.503604
3502.521047	808335.806076	44.508609
3502.964783	808294.470420	44.513613
3502.866998	808261.211707	44.518618
3502.694568	808232.032639	44.523623
3502.722633	808187.285383	44.528628
3502.964405	808151.666883	44.533633
3503.095950	808107.784177	44.538637
3502.822570	808066.075219	44.543642
3502.767223	808023.349929	44.548647
3502.750163	807979.735919	44.553652
3502.515685	807951.546029	44.558657
3502.883500	807908.064179	44.563661
3502.780440	807886.713549	44.568666
3502.660361	807831.745556	44.573671
3503.100625	807796.974660	44.578676
3502.807627	807760.511049	44.583681
3503.032826	807718.668804	44.588685
3502.746520	807679.900196	44.593690
3502.919493	807639.830435	44.598695
3502.853372	807603.965739	44.603700
3502.613207	807561.218988	44.608705
3502.771241	807519.631642	44.613709
3502.727073	807484.448857	44.618714
3502.708140	807442.694152	44.623719
3502.926092	807412.810095	44.628724
3502.982204	807364.082834	44.633729
3503.091345	807320.198745	44.638733
3502.737917	807282.272146	44.643738
3503.025295	807241.200933	44.648743
3502.948678	807212.099730	44.653748
3502.619581	807179.412989	44.658753
3502.971019	807128.429766	44.663757
3502.891716	807090.996091	44.668762
3502.839468	807044.882161	44.673767
3502.910647	807002.374692	44.678772
3502.743698	806967.503558	44.683777
3502.878827	806932.876567	44.688781
3502.704152	806887.516976	44.693786
3502.914287	806855.769167	44.698791
3502.735557	806816.879888	44.703796
3502.763278	806779.181785	44.708801
3502.989694	806742.676159	44.713805
3502.587604	806712.548078	44.718810
3502.727487	806660.272756	44.723815
3502.638770	806623.720380	44.728820
3502.729804	806594.539900	44.733825
3502.527119	806555.064860	44.738829
3502.724833	806510.474714	44.743834
3502.488511	806477.573244	44.748839
3502.669612	806449.994926	44.753844
3502.215237	806418.795744	44.758849
3502.465140	806377.382376	44.763853
3502.304387	806357.605081	44.768858
3502.556808	806321.190957	44.773863
3502.540226	806281.095429	44.778868
3502.333361	806243.383999	44.783873
3502.460472	806227.431510	44.788877
3502.312509	806204.269245	44.793882
3502.731108	806162.826783	44.798887
3502.666799	806117.688994	44.803892
3502.318698	806093.235752	44.808897
3502.718392	806064.443346	44.813901
3502.242984	806028.882910	44.818906
3502.544133	805999.910382	44.823911
3502.642559	805970.627976	44.828916
3502.633849	805934.597974	44.833921
3502.317916	805897.637944	44.838925
3502.435566	805861.096507	44.843930
3502.488719	805828.928586	44.848935
3502.318646	805800.425041	44.853940
3502.284169	805777.977985	44.858945
3502.848649	805746.264689	44.863949
3502.285230	805701.745651	44.868954
3502.654023	805668.201312	44.873959
3502.499010	805626.997190	44.878964
3502.371877	805608.830006	44.883969
3502.584269	805573.987300	44.888973
3502.545598	805556.589805	44.893978
3502.307941	805503.191230	44.898983
3502.430718	805480.423133	44.903988
3502.170743	805450.069955	44.908993
3502.271833	805418.382466	44.913997
3502.448917	805392.320363	44.919002
3502.326526	805360.767482	44.924007
3502.373360	805325.117332	44.929012
3502.002959	805295.615121	44.934017
3502.791073	805260.921100	44.939021
3502.336740	805237.168677	44.944026
3502.405412	805210.535413	44.949031
3502.427397	805184.792243	44.954036
3502.282370	805157.507590	44.959041
3502.704041	805117.284002	44.964045
3502.322833	805089.792851	44.969050
3502.133184	805055.700152	44.974055
3502.452411	805037.850138	44.979060
3502.291382	804994.338830	44.984065
3502.196385	804975.135050	44.989069
3502.344251	804953.194570	44.994074
3502.162706	804927.385906	44.999079
3502.295286	804883.237157	45.004084
3502.238243	804861.035963	45.009089
3502.308511	804823.172974	45.014093
3502.327377	804804.440261	45.019098
3502.407474	804761.476113	45.024103
3502.539788	804736.987889	45.029108
3502.228388	804717.966136	45.034113
3502.808873	804679.626039	45.039117
3502.317261	804653.279050	45.044122
3502.444323	804613.248144	45.049127
3502.411209	804576.332436	45.054132
3502.431534	804553.431044	45.059137
3502.318889	804528.001783	45.064141
3502.357113	804487.445419	45.069146
3502.215933	804462.167715	45.074151
3502.502064	804426.571529	45.079156
3502.334715	804414.831179	45.084161
3502.538060	804370.520369	45.089165
3502.275090	804354.823928	45.094170
3502.431277	804318.316946	45.099175
3502.480167	804298.155910	45.104180
3502.481878	804264.616156	45.109185
3502.437875	804228.533958	45.114189
3502.307769	804213.894069	45.119194
3502.393820	804175.289378	45.124199
3502.036649	804138.473741	45.129204
3502.104678	804121.300197	45.134209
3502.349953	804084.286936	45.139213
3502.118031	804046.028124	45.144218
3502.317816	804039.424471	45.149223
3501.962451	804005.746139	45.154228
3502.042594	803983.274316	45.159233
3502.324551	803964.446924	45.164237
3501.675145	803924.883193	45.169242
3502.231170	803913.807390	45.174247
3502.168185	803889.838693	45.179252
3502.140539	803870.424571	45.184257
3502.295221	803842.398775	45.189261
3502.367046	803812.621155	45.194266
3502.277351	803794.197797	45.199271
3502.680314	803752.939505	45.204276
3502.260971	803742.759707	45.209281
3502.525984	803693.138225	45.214285
3502.445703	803665.346575	45.219290
3502.530199	803633.016067	45.224295
3502.536913	803607.563727	45.229300
3502.549655	803565.142620	45.234305
3502.929538	803531.438896	45.239309
3502.575183	803501.779188	45.244314
3502.544199	803451.518172	45.249319
3502.623277	803429.682239	45.254324
3502.629024	803401.777268	45.259329
3502.668549	803377.201402	45.264333
3502.355938	803336.843170	45.269338
3502.019110	803308.700017	45.274343
3502.446361	803271.112940	45.279348
3502.093802	803264.844760	45.284353
3502.447536	803225.062666	45.289357
3502.431424	803209.715263	45.294362
3502.289600	803185.413803	45.299367
3502.536988	803148.787497	45.304372
3502.506567	803126.723431	45.309377
3502.776486	803084.355069	45.314381
3502.625811	803056.817772	45.319386
3502.387381	803024.831870	45.324391
3502.659863	802983.149071	45.329396
3502.604399	802959.862503	45.334401
3502.215192	802907.939997	45.339405
3502.341939	802884.377929	45.344410
3502.355355	802858.235089	45.349415
3502.555032	802833.189491	45.354420
3502.363071	802803.254783	45.359425
3502.855257	802766.831338	45.364429
3502.690479	802742.384957	45.369434
3502.634403	802699.136073	45.374439
3502.851970	802657.754629	45.379444
3502.624715	802631.356304	45.384449
3503.017680	802604.267131	45.389453
3502.785467	802553.395103	45.394458
3502.502854	802527.643109	45.399463
3502.510111	802491.249060	45.404468
3502.410009	802457.913453	45.409473
3502.412085	802421.863224	45.414477
3502.565102	802393.096085	45.419482
3502.199853	802361.667520	45.424487
3502.863219	802326.341653	45.429492
3502.620010	802301.268998	45.434497
3502.545118	802265.966363	45.439501
3502.260267	802248.502945	45.444506
3502.659301	802207.971782	45.449511
3502.528786	802178.612824	45.454516
3502.286830	802151.969834	45.459521
3502.631039	802116.499281	45.464525
3502.285900	802087.567696	45.469530
3502.496652	802061.732669	45.474535
3502.568680	802028.709976	45.479540
3502.550877	801987.853796	45.484545
3502.295289	801957.386333	45.489549
3502.167678	801940.926298	45.494554
3502.338982	801898.812153	45.499559
3502.170694	801874.461369	45.504564
3502.369902	801846.861581	45.509569
3502.323138	801820.185147	45.514573
3502.644002	801795.606334	45.519578
3502.647356	801763.819993	45.524583
3502.400055	801722.754793	45.529588
3502.419259	801696.655644	45.534593
3502.480235	801655.244932	45.539597
3502.369614	801645.354517	45.544602
3501.987267	801610.785929	45.549607
3502.356982	801585.953055	45.554612
3502.158119	801557.338516	45.559617
3502.370426	801530.127735	45.564621
3502.660699	801504.571846	45.569626
3502.328465	801468.816987	45.574631
3502.571867	801444.102524	45.579636
3502.245358	801430.028665	45.584641
3502.573384	801382.195187	45.589645
3502.364526	801360.890692	45.594650
3502.477327	801328.103205	45.599655
3502.723776	801305.300910	45.604660
3502.289000	801272.161877	45.609665
3502.642943	801233.692776	45.614669
3502.583818	801212.363152	45.619674
3502.231369	801182.104445	45.624679
3502.474843	801136.392629	45.629684
3502.613062	801116.011329	45.634689
3502.637762	801080.931504	45.639693
3502.825775	801048.424642	45.644698
3502.243629	801013.689749	45.649703
3502.688010	800987.027286	45.654708
3502.328447	800969.180467	45.659713
3502.642226	800926.938806	45.664717
3502.297918	800884.020377	45.669722
3502.373077	800872.037778	45.674727
3502.687332	800828.421791	45.679732
3502.375838	800800.411378	45.684737
3502.488522	800759.967964	45.689741
3502.244340	800733.761394	45.694746
3502.311763	800707.061844	45.699751
3502.460088	800677.895854	45.704756
3502.085695	800659.020412	45.709761
3502.553612	800625.091754	45.714765
3502.468805	800597.631894	45.719770
3502.134471	800572.567963	45.724775
3502.580349	800530.253054	45.729780
3502.185308	800517.856702	45.734785
3502.416858	800465.077586	45.739789
3502.680917	800444.967946	45.744794
3502.399706	800407.629203	45.749799
3502.830375	800381.506353	45.754804
3502.582276	800352.747745	45.759809
3502.770919	800325.487063	45.764813
3502.518997	800273.473023	45.769818
3502.359669	800178.758062	45.774823
3502.573877	800035.406375	45.779828
3502.628163	799834.082153	45.784833
3502.468642	799550.353330	45.789837
3501.941614	799249.008168	45.794842
3501.876304	798878.675837	45.799847
3502.137011	798439.662135	45.804852
3501.768227	797952.086867	45.809857
3501.658486	797383.398436	45.814861
3501.467279	796770.056347	45.819866
3500.908630	796090.053483	45.824871
3500.544348	795349.906073	45.829876
3500.364483	794558.484495	45.834881
3500.189461	793688.250807	45.839885
3500.061022	792758.864513	45.844890
3499.385101	791762.442397	45.849895
3499.142146	790692.604336	45.854900
3498.783983	789560.709485	45.859905
3498.272152	788352.580685	45.864909
3498.061445	787085.407294	45.869914
3497.218888	785752.429155	45.874919
3496.921746	784335.565919	45.879924
3496.173182	782860.213756	45.884929
3495.646409	781302.416382	45.889933
3495.213493	779689.894824	45.894938
3494.688483	777992.720352	45.899943
3494.288693	776209.617826	45.904948
3493.385908	774377.019291	45.909953
3492.585823	772458.686095	45.914957
3491.943762	770457.598858	45.919962
3490.959542	768399.303234	45.924967
3490.764754	766262.962236	45.929972
3489.520904	764069.130746	45.934977
3488.820484	761784.253880	45.939981
3487.656428	759449.716630	45.944986
3486.819730	757037.904690	45.949991
3486.498659	754555.926371	45.954996
3485.419227	752006.842139	45.960001
3484.593123	749374.515198	45.965005
3483.371341	746678.050441	45.970010
3482.303830	743908.446994	45.975015
3481.270044	741082.914626	45.980020
3480.020080	738187.241995	45.985025
3478.977059	735225.744682	45.990029
3477.876236	732206.372858	45.995034
3476.507626	729121.674893	46.000039
3475.819523	725970.438070	46.005044
3474.311579	722745.952264	46.010049
3473.142214	719455.537965	46.015053
3471.740998	716107.705026	46.020058
3470.496432	712697.815726	46.025063
3469.269320	709215.900007	46.030068
3467.710278	705684.688886	46.035073
3466.379596	702087.495528	46.040077
3464.779475	698420.406703	46.045082
3463.482465	694702.600933	46.050087
3462.438131	690919.460148	46.055092
3460.646356	687085.765819	46.060097
3459.013503	683172.887017	46.065101
3457.340430	679208.221797	46.070106
3455.811541	675192.239411	46.075111
3454.386366	671104.705370	46.080116
3452.353746	666978.087311	46.085121
3451.014759	662782.746551	46.090125
3449.439035	658534.295088	46.095130
3447.190533	654221.568856	46.100135
3445.792754	649843.405707	46.105140
3443.728477	645425.739694	46.110145
3442.153865	640942.395509	46.115149
3440.384473	636413.539792	46.120154
3438.305184	631810.124273	46.125159
3436.772018	627163.387576	46.130164
3434.545421	622471.802088	46.135169
3433.044094	617731.846226	46.140173
3431.243829	612927.508825	46.145178
3428.936795	608063.637449	46.150183
3427.031508	603150.476320	46.155188
3424.478998	598192.736780	46.160193
3422.614105	593179.676627	46.165197
3420.427647	588124.240945	46.170202
3418.383302	583002.705853	46.175207
3416.429967	577847.171990	46.180212
3414.123328	572636.121605	46.185217
3411.893278	567378.715260	46.190221
3409.246094	562066.405336	46.195226
3407.010110	556714.192410	46.200231
3404.967212	551305.675572	46.205236
3402.352178	545862.030773	46.210241
3400.062276	540377.159856	46.215245
3397.804480	534842.932773	46.220250
3395.343975	529265.736246	46.225255
3392.813416	523632.012340	46.230260
3390.317371	517969.106162	46.235265
3387.788027	512246.471786	46.240269
3385.342971	506497.942901	46.245274
3382.361325	500710.242892	46.250279
3380.149096	494876.285755	46.255284
3377.354516	489015.831061	46.260289
3374.471913	483088.528298	46.265293
3371.483317	477146.878199	46.270298
3368.673530	471162.254612	46.275303
3366.230374	465144.419707	46.280308
3362.967110	459101.652817	46.285313
3360.151528	453005.183769	46.290317
3357.532189	446893.201329	46.295322
3354.385297	440742.534195	46.300327
3351.334528	434554.932626	46.305332
3348.379688	428347.784974	46.310337
3345.286750	422098.633169	46.315341
3342.087286	415836.700707	46.320346
3338.850381	409537.291776	46.325351
3336.108924	403214.402140	46.330356
3332.647139	396872.395520	46.335361
3329.209570	390500.983822	46.340365
3325.889595	384114.838821	46.345370
3322.564956	377699.722939	46.350375
3319.482801	371256.788556	46.355380
3315.556803	364794.913023	46.360385
3312.001384	358315.174017	46.365389
3308.953394	351820.813084	46.370394
3305.047927	345316.441770	46.375399
3301.441740	338791.804523	46.380404
3298.025222	332259.756259	46.385409
3294.463662	325716.472607	46.390413
3290.610767	319163.417384	46.395418
3286.931326	312604.246149	46.400423
3282.896953	306027.070408	46.405428
3278.935127	299457.526252	46.410433
3275.524777	292874.266507	46.415437
3271.465886	286273.329040	46.420442
3267.359154	279691.889593	46.425447
3263.376330	273086.951649	46.430452
3259.057836	266506.437485	46.435457
3255.015976	259911.019615	46.440461
3250.775397	253324.225993	46.445466
3246.594283	246743.562508	46.450471
3242.638117	240161.329239	46.455476
3238.525949	233597.038733	46.460481
3234.243009	227046.584440	46.465485
3230.133913	220423.450382	46.470490
3225.900083	213846.244275	46.475495
3221.603636	207302.515479	46.480500
3216.758396	200781.750976	46.485505
3212.194190	194268.093567	46.490509
3207.709453	187772.866894	46.495514
3203.170142	181302.707764	46.500519
3198.654367	174839.606758	46.505524
3193.861699	168414.857678	46.510529
3189.468828	161985.927563	46.515533
3184.635988	155614.830267	46.520538
3179.648900	149237.952147	46.525543
3175.374491	142899.091141	46.530548
3170.187353	136593.143520	46.535553
3164.955610	130295.152307	46.540557
3160.432793	124042.685993	46.545562
3154.752683	117831.931628	46.550567
3149.698554	111650.436218	46.555572
3144.252797	105514.127189	46.560577
3139.090877	99415.697115	46.565581
3133.658827	93363.847254	46.570586
3127.741840	87350.647664	46.575591
3122.416441	81401.862886	46.580596
3116.265102	75514.331755	46.585601
3110.640189	69654.858017	46.590605
3104.332118	63882.697500	46.595610
3097.812077	58174.846102	46.600615
3091.525318	52524.712821	46.605620
3083.826480	46978.689619	46.610625
3074.943516	41551.208997	46.615629
3060.129480	36407.203381	46.620634
3043.054502	31484.115508	46.625639
3026.816373	26750.594446	46.630644
3011.047369	22288.121485	46.635649
2995.544126	18074.646599	46.640653
2978.517189	14230.111965	46.645658
2958.127613	10792.763345	46.650663
2935.907767	7748.992588	46.655668
2913.754764	5106.758372	46.660673
2893.195677	2851.102573	46.665677
2874.350790	998.041102	46.670682
2828.697962	287.805338	46.675687
2780.150257	283.920792	46.680692
2759.579915	289.084745	46.685697
2763.153582	284.735435	46.690701
2779.163618	286.865663	46.695706
2797.469262	275.992396	46.700711
2811.513021	275.238358	46.705716
2819.011472	269.430856	46.710721
2820.447632	281.687768	46.715725
2818.356675	271.917487	46.720730
2814.519730	272.731815	46.725735
2810.399552	273.020979	46.730740
2806.908800	265.678475	46.735745
2803.636269	267.961850	46.740749
2801.167310	265.942406	46.745754
2798.539278	268.218513	46.750759
2795.762262	253.352009	46.755764
2792.953143	264.807962	46.760769
2790.694409	256.319299	46.765773
2787.711506	256.494249	46.770778
2784.193544	262.876274	46.775783
2781.360304	257.220728	46.780788
2778.331114	262.480934	46.785793
2775.405989	262.319164	46.790797
2772.241835	245.285411	46.795802
2769.061280	257.073014	46.800807
2765.519721	251.816155	46.805812
2762.222322	257.833028	46.810817
2759.235344	256.669108	46.815821
2756.164735	253.068792	46.820826
2752.869336	255.327158	46.825831
2749.883421	255.937964	46.830836
2746.472138	247.983273	46.835841
2742.941270	249.296156	46.840845
2739.991635	240.809835	46.845850
2736.383133	246.692945	46.850855
2733.232556	239.822468	46.855860
2729.571448	240.090415	46.860865
2726.119801	242.376157	46.865869
2722.855121	239.245987	46.870874
2719.282027	243.764370	46.875879
2716.357748	240.944302	46.880884
2712.946971	240.592348	46.885889
2709.696198	242.588016	46.890893
2706.238918	240.259271	46.895898
2702.498338	244.050667	46.900903
2699.546749	236.157118	46.905908
2696.145418	240.833857	46.910913
2692.566493	241.092217	46.915917
2689.270704	231.755678	46.920922
2685.495230	232.763616	46.925927
2681.834412	233.663832	46.930932
2678.662725	235.761321	46.935937
2675.497803	239.359071	46.940941
2672.031458	232.100280	46.945946
2668.327918	237.756779	46.950951
2665.583897	235.267738	46.955956
2662.428719	233.912982	46.960961
2658.509943	231.571625	46.965965
2655.053739	227.244856	46.970970
2651.433192	230.084235	46.975975
2648.139908	223.791115	46.980980
2644.241403	230.966967	46.985985
2641.122554	230.118528	46.990989
2637.814088	225.956050	46.995994
2633.732999	232.049035	47.000999
2630.181650	231.765329	47.006004
2627.138849	229.948427	47.011009
2624.080267	231.865069	47.016013
2620.726713	221.534443	47.021018
2617.332345	218.453775	47.026023
2614.081822	219.236204	47.031028
2610.122908	224.468368	47.036033
2606.230982	227.074707	47.041037
2603.073478	216.325350	47.046042
2599.624156	230.082634	47.051047
2596.267809	217.029970	47.056052
2592.835674	220.079840	47.061057
2589.135103	220.264414	47.066061
2585.425004	220.982201	47.071066
2581.862754	232.841162	47.076071
2578.741560	217.344901	47.081076
2575.767005	218.750403	47.086081
2572.093383	221.454931	47.091085
2568.954874	217.698211	47.096090
2565.076872	222.116243	47.101095
2561.829307	216.377868	47.106100
2557.883110	223.357794	47.111105
2554.507773	214.371556	47.116109
2550.880232	209.023688	47.121114
2547.170846	224.945334	47.126119
2544.520492	213.172780	47.131124
2541.056708	216.854662	47.136129
2537.743451	221.558204	47.141133
2533.882010	209.224595	47.146138
2529.625634	218.396291	47.151143
2526.661120	213.293829	47.156148
2523.203079	216.948726	47.161153
2519.938915	221.100896	47.166157
2516.310443	209.509534	47.171162
2512.885303	222.625654	47.176167
2509.692609	217.939757	47.181172
2506.263761	222.606944	47.186177
2502.201354	218.789038	47.191181
2498.823079	214.880716	47.196186
2495.287932	221.018278	47.201191
2492.107972	212.954183	47.206196
2488.485550	214.707424	47.211201
2484.646383	216.465262	47.216205
2481.425569	207.757091	47.221210
2478.046242	211.674709	47.226215
2474.559214	208.392956	47.231220
2470.922413	212.370443	47.236225
2467.536955	213.398037	47.241229
2463.781256	209.296088	47.246234
2460.438285	213.001693	47.251239
2457.147693	208.907243	47.256244
2453.659540	209.132241	47.261249
2450.231310	209.636849	47.266253
2447.416999	201.913040	47.271258
2443.525450	207.259513	47.276263
2439.498530	208.222702	47.281268
2435.812647	206.745922	47.286273
2432.543763	208.128257	47.291277
2429.107378	211.861537	47.296282
2425.266432	211.113880	47.301287
2422.094450	209.028935	47.306292
2418.790842	206.010590	47.311297
2415.129752	205.214308	47.316301
2412.002971	208.460962	47.321306
2408.420120	208.919881	47.326311
2404.969414	198.770454	47.331316
2401.154390	195.343784	47.336321
2397.914054	201.157251	47.341325
2394.511572	196.964691	47.346330
2390.729611	203.234031	47.351335
2386.817974	197.513843	47.356340
2383.652405	199.887566	47.361345
2380.275821	199.973425	47.366349
2377.176513	193.258550	47.371354
2373.675425	198.673032	47.376359
2370.221264	192.143630	47.381364
2366.479118	197.525485	47.386369
2362.446874	201.259881	47.391373
2359.149038	196.835957	47.396378
2355.961344	197.930044	47.401383
2352.524595	199.328696	47.406388
2349.008191	199.972846	47.411393
2345.215646	203.854567	47.416397
2342.122608	197.379633	47.421402
2337.965783	203.655046	47.426407
2335.116819	190.453340	47.431412
2331.305560	200.832434	47.436417
2327.732963	213.455960	47.441421
2324.543334	197.142587	47.446426
2321.087124	201.445575	47.451431
2317.464339	197.962174	47.456436
2313.559126	194.743859	47.461441
2309.998914	197.122786	47.466445
2307.211799	189.608107	47.471450
2303.467648	201.356734	47.476455
2300.040408	199.031618	47.481460
2296.163678	189.925901	47.486465
2292.930489	184.998992	47.491469
2289.710629	186.969293	47.496474
2286.111898	193.048015	47.501479
2282.912751	195.271444	47.506484
2278.922191	190.375845	47.511489
2275.222677	199.432306	47.516493
2271.779516	185.551624	47.521498
2268.437314	193.049506	47.526503
2265.107396	183.319738	47.531508
2261.460724	184.529919	47.536513
2257.825429	188.498222	47.541517
2254.289267	197.651064	47.546522
2251.001022	195.827764	47.551527
2247.354344	186.711737	47.556532
2244.275738	192.124039	47.561537
2240.603266	190.437002	47.566541
2237.399764	183.466907	47.571546
2233.299272	192.932769	47.576551
2230.002362	197.000137	47.581556
2226.619746	199.689818	47.586561
2222.890831	199.129848	47.591565
2219.489566	192.399817	47.596570
2215.960287	190.163838	47.601575
2212.618275	190.324620	47.606580
2208.871339	183.384872	47.611585
2205.500269	196.524578	47.616589
2201.798196	188.593290	47.621594
2198.322711	196.860550	47.626599
2194.978767	180.989563	47.631604
2191.678268	193.425946	47.636609
2188.024619	188.720092	47.641613
2185.045555	185.389025	47.646618
2181.241242	193.936740	47.651623
2177.581803	183.443673	47.656628
2174.088976	177.537304	47.661633
2170.356806	183.146166	47.666637
2167.157667	181.345510	47.671642
2163.009410	192.558467	47.676647
2159.595646	183.319992	47.681652
2156.621943	180.843331	47.686657
2153.165531	184.423012	47.691661
2149.510215	178.243141	47.696666
2145.914587	183.651671	47.701671
2142.642647	184.236854	47.706676
2139.002370	179.098634	47.711681
2135.530222	181.365260	47.716685
2132.249952	176.749752	47.721690
2128.662189	182.324733	47.726695
2125.050338	181.758929	47.731700
2121.674746	180.545124	47.736705
2117.875921	184.463369	47.741709
2114.541472	174.674876	47.746714
2110.773559	178.877321	47.751719
2107.450423	184.295149	47.756724
2104.087389	180.153721	47.761729
2100.504299	183.715677	47.766733
2097.247142	171.662396	47.771738
2093.556645	179.892598	47.776743
2090.114747	176.007722	47.781748
2086.833963	180.786884	47.786753
2083.034051	177.299966	47.791757
2079.801633	169.670522	47.796762
2075.743415	176.623102	47.801767
2072.288264	171.413123	47.806772
2069.002450	178.013583	47.811777
2065.514829	179.445896	47.816781
2062.399257	174.184779	47.821786
2058.343172	174.990881	47.826791
2054.829359	174.355264	47.831796
2051.387697	171.593439	47.836801
2048.010043	178.876086	47.841805
2044.528773	176.134225	47.846810
2040.779793	179.718487	47.851815
2037.676059	176.960855	47.856820
2034.358353	168.170770	47.861825
2030.516316	173.661905	47.866829
2027.006533	175.465942	47.871834
2023.236114	178.814780	47.876839
2019.871347	171.865562	47.881844
2016.593484	172.446085	47.886849
2013.041113	177.479917	47.891853
2009.918658	177.745479	47.896858
2006.187319	183.767944	47.901863
2002.394379	171.834996	47.906868
1999.144985	173.756881	47.911873
1995.367353	176.838549	47.916877
1991.958224	168.938203	47.921882
1988.428609	174.536630	47.926887
1985.023018	174.928300	47.931892
1981.438605	172.854545	47.936897
1977.995950	176.403061	47.941901
1974.460366	177.566098	47.946906
1971.003154	173.635494	47.951911
1967.580096	177.958891	47.956916
1964.153539	165.748990	47.961921
1960.607044	171.225307	47.966925
1957.342527	165.843823	47.971930
1953.778464	174.691628	47.976935
1949.944357	170.799214	47.981940
1946.570622	170.428065	47.986945
1942.882525	174.597715	47.991949
1939.467205	170.848084	47.996954
1935.531939	170.462928	48.001959
1932.242825	169.011588	48.006964
1929.010177	172.581693	48.011969
1925.667807	168.728656	48.016973
1922.585498	157.167427	48.021978
1918.370295	169.097094	48.026983
1914.843969	172.872007	48.031988
1911.370850	164.409027	48.036993
1907.733666	167.711867	48.041997
1904.686097	171.892178	48.047002
1901.388159	170.932508	48.052007
1897.956754	161.364458	48.057012
1893.999068	163.428071	48.062017
1890.731520	169.790984	48.067021
1886.899067	171.645459	48.072026
1883.174303	172.601621	48.077031
1879.915665	166.845660	48.082036
1876.724055	161.163094	48.087041
1872.948832	173.658120	48.092045
1869.703281	165.999827	48.097050
1866.177877	164.635321	48.102055
1862.002522	165.260792	48.107060
1858.894124	165.520973	48.112065
1855.159650	171.223384	48.117069
1852.114544	160.332145	48.122074
1848.494049	166.876721	48.127079
1845.186995	163.295370	48.132084
1841.552953	154.776350	48.137089
1837.560035	168.570127	48.142093
1834.643418	159.469051	48.147098
1830.973271	164.208296	48.152103
1827.625775	157.971341	48.157108
1824.059455	159.395315	48.162113
1820.044776	167.659121	48.167117
1816.423332	155.533251	48.172122
1813.571023	163.377909	48.177127
1810.098079	164.142946	48.182132
1806.762198	157.947898	48.187137
1802.913588	169.269281	48.192141
1799.819107	168.014796	48.197146
1795.928845	167.782166	48.202151
1792.326235	172.444965	48.207156
1788.871926	158.391923	48.212161
1785.385112	168.345984	48.217165
1782.127251	158.838559	48.222170
1778.661300	166.348097	48.227175
1774.719443	162.476792	48.232180
1771.346645	154.857559	48.237185
1767.942026	163.090280	48.242189
1764.359045	156.329467	48.247194
1760.895358	168.015711	48.252199
1757.454469	162.515510	48.257204
1753.779394	162.239669	48.262209
1750.371237	170.563371	48.267213
1746.984213	158.011655	48.272218
1743.725423	165.125860	48.277223
1739.714812	154.909470	48.282228
1736.435501	151.470044	48.287233
1732.509700	157.474107	48.292237
1729.321174	153.411885	48.297242
1725.861455	155.460854	48.302247
1722.684605	159.966333	48.307252
1719.029978	155.489947	48.312257
1715.280551	153.523191	48.317261
1711.580196	153.785559	48.322266
1708.349718	161.629404	48.327271
1704.732693	155.312159	48.332276
1701.667626	158.715203	48.337281
1698.095483	158.918114	48.342285
1694.617680	147.876092	48.347290
1690.861419	150.098206	48.352295
1687.416204	158.283217	48.357300
1683.853728	148.293786	48.362305
1680.551261	159.828127	48.367309
1676.823513	148.747888	48.372314
1673.377784	156.745916	48.377319
1669.709572	159.367909	48.382324
1666.434723	159.346489	48.387329
1662.736288	156.155351	48.392333
1659.445639	142.427055	48.397338
1655.582534	156.493732	48.402343
1652.144438	151.119651	48.407348
1649.052465	149.251330	48.412353
1645.155798	159.546507	48.417357
1641.859687	144.789216	48.422362
1638.387125	145.013609	48.427367
1634.886995	148.308209	48.432372
1631.460145	142.124190	48.437377
1627.662342	154.520677	48.442381
1624.260453	160.196519	48.447386
1620.719567	153.705145	48.452391
1617.213202	152.099103	48.457396
1614.381430	146.289789	48.462401
1609.956917	154.333156	48.467405
1606.457766	145.378040	48.472410
1603.343359	149.922805	48.477415
1599.896676	147.786929	48.482420
1596.428844	142.106015	48.487425
1592.314418	147.431723	48.492429
1589.354655	148.034373	48.497434
1585.756494	147.878567	48.502439
1582.486538	151.083864	48.507444
1578.999757	152.709383	48.512449
1575.154147	157.446627	48.517453
1571.996315	156.915354	48.522458
1568.492222	152.535581	48.527463
1564.788087	156.144558	48.532468
1561.356465	151.475556	48.537473
1557.270888	154.935235	48.542477
1553.966272	148.212077	48.547482
1550.765422	141.980515	48.552487
1547.402892	144.821453	48.557492
1543.791990	140.875540	48.562497
1540.290941	150.594503	48.567501
1536.851207	143.863694	48.572506
1533.477447	152.758265	48.577511
1529.859544	155.654442	48.582516
1526.260044	149.863123	48.587521
1522.657033	158.278760	48.592525
1519.513170	144.577435	48.597530
1515.820940	146.007842	48.602535
1511.895924	150.619527	48.607540
1508.421263	148.512419	48.612545
1504.728750	157.721949	48.617549
1501.842658	144.538481	48.622554
1498.500213	148.927210	48.627559
1494.623814	145.750232	48.632564
1491.334661	145.684924	48.637569
1487.441539	155.195405	48.642573
1484.426945	156.464713	48.647578
1481.203050	159.652008	48.652583
1477.247478	161.468743	48.657588
1473.804710	155.446727	48.662593
1470.131474	164.942002	48.667597
1466.571873	141.164674	48.672602
1463.124368	151.407454	48.677607
1459.419495	152.012359	48.682612
1456.363955	140.362030	48.687617
1452.794010	156.099799	48.692621
1449.157911	146.442034	48.697626
1445.504592	148.095767	48.702631
1441.774712	146.895231	48.707636
1438.935395	139.073254	48.712641
1434.879366	149.546668	48.717645
1431.842581	135.952049	48.722650
1428.249722	150.362177	48.727655
1424.740357	153.389484	48.732660
1421.580060	142.564987	48.737665
1417.364570	146.468556	48.742669
1413.999676	141.218932	48.747674
1410.695923	156.258753	48.752679
1407.062804	159.155367	48.757684
1403.872469	142.651136	48.762689
1399.784291	149.599321	48.767693
1396.651741	145.285563	48.772698
1393.157675	150.049502	48.777703
1389.471166	151.173189	48.782708
1386.400502	142.684989	48.787713
1382.395247	152.136328	48.792717
1379.228985	143.197230	48.797722
1375.672058	152.234461	48.802727
1372.267796	148.439833	48.807732
1368.797651	157.992185	48.812737
1364.860918	152.883486	48.817741
1361.748546	147.566310	48.822746
1358.590236	141.697477	48.827751
1354.356112	146.071476	48.832756
1350.747348	143.807474	48.837761
1347.197869	151.830362	48.842765
1343.963221	143.914542	48.847770
1340.572973	140.317133	48.852775
1336.965992	139.717786	48.857780
1333.916818	142.593313	48.862785
1330.077635	145.056354	48.867789
1326.568092	145.076336	48.872794
1322.967345	148.811476	48.877799
1319.592961	142.616865	48.882804
1316.238974	139.236868	48.887809
1312.426615	144.585102	48.892813
1308.748281	147.187336	48.897818
1305.681315	146.786467	48.902823
1302.197974	148.932001	48.907828
1298.950274	146.588228	48.912833
1294.958354	146.602525	48.917837
1291.307348	148.960490	48.922842
1288.016767	151.811818	48.927847
1284.272689	154.503678	48.932852
1281.049749	141.920716	48.937857
1277.600015	153.064829	48.942861
1274.205793	146.544768	48.947866
1270.714681	151.989712	48.952871
1267.040801	146.493694	48.957876
1263.559559	150.464281	48.962881
1259.872000	148.228376	48.967885
1256.817493	146.466022	48.972890
1253.018789	151.705683	48.977895
1249.404128	147.174540	48.982900
1245.924206	145.487060	48.987905
1242.598775	146.772979	48.992909
1239.247959	148.585647	48.997914
1235.289428	147.314940	49.002919
1231.846784	151.551495	49.007924
1228.435694	146.588490	49.012929
1224.844768	151.312320	49.017933
1221.687655	143.451270	49.022938
1218.151054	140.111798	49.027943
1214.272547	156.897870	49.032948
1211.030613	143.508824	49.037953
1207.261016	144.392221	49.042957
1204.373154	141.670133	49.047962
1200.480578	145.100771	49.052967
1196.498474	145.489064	49.057972
1193.578049	145.026156	49.062977
1189.787565	147.092111	49.067981
1186.562472	148.411211	49.072986
1182.951217	148.807470	49.077991
1179.238832	155.537418	49.082996
1175.987163	137.294729	49.088001
1172.633392	153.125195	49.093005
1169.117142	142.856647	49.098010
1165.100353	145.830097	49.103015
1161.234862	139.021591	49.108020
1158.438714	134.855848	49.113025
1155.218350	150.367668	49.118029
1151.285299	142.985431	49.123034
1147.971993	139.194296	49.128039
1144.494281	145.691485	49.133044
1141.131519	138.838952	49.138049
1137.346746	147.852445	49.143053
1133.965477	142.730466	49.148058
1130.349772	140.888121	49.153063
1126.892885	133.389888	49.158068
1123.601984	135.716464	49.163073
1119.651651	132.927378	49.168077
1116.033443	141.105248	49.173082
1113.367208	136.022145	49.178087
1109.632794	139.853348	49.183092
1106.101570	136.577017	49.188097
1102.074455	140.170484	49.193101
1098.728387	138.893551	49.198106
1095.149847	139.031090	49.203111
1092.002472	148.121170	49.208116
1088.651252	139.675050	49.213121
1084.357889	142.726268	49.218125
1081.258586	140.159796	49.223130
1077.935228	139.934285	49.228135
1074.310269	141.158751	49.233140
1071.022201	137.623199	49.238145
1067.509928	150.501524	49.243149
1063.726960	138.281900	49.248154
1060.514722	142.721623	49.253159
1056.580944	151.846645	49.258164
1053.585833	149.094635	49.263169
1049.887458	150.835654	49.268173
1046.290397	140.057834	49.273178
1042.977596	142.664164	49.278183
1039.430530	140.436984	49.283188
1035.871040	138.592328	49.288193
1032.194023	147.404360	49.293197
1028.384902	143.999598	49.298202
1024.995860	139.444955	49.303207
1021.670193	148.500624	49.308212
1018.332426	140.009121	49.313217
1014.616954	144.041511	49.318221
1011.481671	143.086572	49.323226
1007.781857	140.959863	49.328231
1004.007186	144.292823	49.333236
1000.792638	141.836833	49.338241
997.307676	148.049187	49.343245
993.870407	139.592511	49.348250
989.977704	132.090885	49.353255
986.388224	147.654165	49.358260
983.621500	137.228487	49.363265
979.757876	146.545813	49.368269
976.486582	142.912047	49.373274
972.690144	136.570249	49.378279
969.294974	137.469081	49.383284
966.105198	133.122088	49.388289
962.206905	137.431621	49.393293
958.765619	136.746369	49.398298
955.249683	136.403610	49.403303
951.524854	148.124654	49.408308
948.242346	132.580336	49.413313
944.799392	133.712053	49.418317
941.241695	140.881912	49.423322
937.795223	133.265689	49.428327
933.947845	139.558543	49.433332
930.678117	136.934130	49.438337
927.393190	135.920132	49.443341
923.787316	139.893421	49.448346
920.479890	130.306900	49.453351
916.747418	137.871543	49.458356
913.200675	139.899386	49.463361
909.321381	135.178657	49.468365
906.087818	136.073897	49.473370
902.611735	133.605193	49.478375
899.079842	144.702748	49.483380
895.791704	135.489178	49.488385
892.004750	137.006000	49.493389
888.888509	133.467824	49.498394
885.007534	137.406918	49.503399
881.439819	140.088084	49.508404
878.304174	133.659185	49.513409
874.399954	138.991776	49.518413
870.906486	139.908124	49.523418
867.669792	131.538763	49.528423
864.404176	135.952121	49.533428
860.990026	130.116515	49.538433
857.249836	142.629114	49.543437
853.622576	138.993343	49.548442
850.199495	133.852070	49.553447
846.376198	134.490084	49.558452
843.097520	127.688818	49.563457
839.623800	139.261249	49.568461
836.257543	137.961214	49.573466
832.565446	133.434359	49.578471
828.907514	138.225806	49.583476
825.711772	137.169505	49.588481
822.070076	135.385390	49.593485
818.966422	140.653098	49.598490
815.311757	136.594661	49.603495
811.525412	140.150723	49.608500
808.149791	124.987014	49.613505
804.430565	140.491548	49.618509
800.851067	138.496077	49.623514
797.767074	138.126000	49.628519
793.841511	142.593909	49.633524
790.664459	131.515973	49.638529
787.117434	135.600402	49.643533
783.543703	136.151406	49.648538
779.672939	134.580255	49.653543
776.521638	138.445509	49.658548
773.336864	127.358803	49.663553
769.430137	132.987899	49.668557
766.132752	129.783480	49.673562
763.143509	127.268695	49.678567
759.022405	130.111155	49.683572
755.481994	133.168760	49.688577
751.898633	132.135194	49.693581
748.265332	133.919762	49.698586
744.762232	121.826245	49.703591
741.369617	127.964297	49.708596
738.236465	123.500962	49.713601
734.454800	138.858002	49.718605
730.847281	127.143484	49.723610
727.987993	120.729376	49.728615
723.839423	133.259891	49.733620
720.210246	127.758939	49.738625
716.808597	135.322285	49.743629
713.709022	128.432492	49.748634
710.606993	124.704828	49.753639
706.360092	130.379791	49.758644
703.008988	125.094323	49.763649
699.067477	125.701897	49.768653
695.825864	128.668675	49.773658
692.880203	126.715452	49.778663
688.836621	135.169427	49.783668
685.632856	127.725210	49.788673
682.091561	130.699544	49.793677
678.186689	127.327319	49.798682
674.844272	121.245569	49.803687
671.246553	129.101668	49.808692
668.043634	124.555404	49.813697
664.860777	136.983824	49.818701
661.200157	128.905983	49.823706
657.504507	125.779775	49.828711
654.014040	134.509511	49.833716
650.476607	125.398968	49.838721
646.877120	131.409498	49.843725
643.445886	126.999300	49.848730
639.994487	114.784258	49.853735
636.555949	125.654989	49.858740
632.685668	117.417691	49.863745
629.003806	129.577822	49.868749
625.816282	130.613452	49.873754
622.853505	128.194831	49.878759
619.075845	127.665747	49.883764
615.742051	124.190215	49.888769
611.615889	131.665513	49.893773
608.152902	129.640073	49.898778
604.582228	123.289882	49.903783
601.251539	129.311621	49.908788
598.079175	125.135688	49.913793
594.462995	129.731754	49.918797
590.878567	123.180200	49.923802
587.616516	125.414373	49.928807
583.566870	125.149563	49.933812
580.137842	123.305997	49.938817
576.824222	128.049745	49.943821
573.054166	131.139962	49.948826
569.959889	129.257788	49.953831
566.284480	135.582670	49.958836
563.077637	127.754849	49.963841
559.448812	126.190042	49.968845
555.846999	125.939957	49.973850
552.402086	115.685045	49.978855
548.844121	125.302387	49.983860
545.499678	119.195427	49.988865
541.648289	123.869130	49.993869
538.271483	129.850986	49.998874
534.708087	117.709430	50.003879
531.096062	121.383101	50.008884
527.884246	119.521593	50.013889
524.161056	130.254996	50.018893
520.741056	129.336474	50.023898
517.392776	123.945315	50.028903
513.958025	128.764406	50.033908
510.598790	114.390181	50.038913
507.139724	124.068739	50.043917
503.363484	132.753517	50.048922
499.853791	122.483714	50.053927
496.240980	127.495281	50.058932
492.714673	119.722755	50.063937
489.230410	128.735150	50.068941
485.883292	128.756147	50.073946
482.427449	121.495698	50.078951
478.631948	132.325364	50.083956
475.280294	130.247470	50.088961
471.771083	118.356701	50.093965
468.058719	119.806282	50.098970
464.802086	120.234423	50.103975
461.058504	125.188330	50.108980
457.647051	114.820419	50.113985
454.438605	130.422202	50.118989
450.929470	132.510686	50.123994
447.711295	120.141978	50.128999
443.481767	127.685636	50.134004
440.064894	127.022211	50.139009
436.757097	126.702256	50.144013
432.931552	123.114469	50.149018
430.292978	121.730637	50.154023
426.565255	123.961481	50.159028
422.664083	111.744118	50.164033
418.824519	120.112253	50.169037
415.588979	123.765741	50.174042
412.125816	121.100533	50.179047
408.348707	128.819965	50.184052
405.248276	125.707755	50.189057
401.736552	126.520537	50.194061
397.564257	132.760050	50.199066
394.834773	129.439242	50.204071
391.412374	129.015349	50.209076
387.902496	126.820446	50.214081
384.078597	126.873663	50.219085
380.618458	124.432548	50.224090
377.167338	125.552241	50.229095
373.763858	132.039665	50.234100
370.337978	122.327198	50.239105
366.903635	120.102841	50.244109
363.095135	123.774828	50.249114
359.611074	122.542028	50.254119
355.948950	131.385436	50.259124
352.716428	122.507087	50.264129
349.142614	131.996761	50.269133
345.869458	122.326132	50.274138
342.433346	119.047332	50.279143
338.600040	124.335871	50.284148
335.269195	125.753202	50.289153
331.744841	120.364899	50.294157
328.019470	123.241512	50.299162
324.822111	125.712628	50.304167
320.906838	135.182079	50.309172
317.406191	118.316201	50.314177
313.932528	120.817469	50.319181
310.519371	122.758554	50.324186
307.528573	124.969148	50.329191
303.581429	132.946508	50.334196
300.099711	125.046200	50.339201
296.528220	127.404820	50.344205
293.377399	127.108326	50.349210
289.124099	120.468847	50.354215
285.844295	128.376012	50.359220
282.562370	125.199611	50.364225
278.971260	125.376401	50.369229
275.336753	121.857977	50.374234
272.388876	124.574758	50.379239
268.683837	139.066560	50.384244
264.974334	124.145507	50.389249
261.807040	127.944887	50.394253
258.149725	124.841302	50.399258
254.439152	113.808935	50.404263
251.013890	123.105363	50.409268
247.881578	124.821221	50.414273
244.148684	132.437955	50.419277
240.247023	127.603751	50.424282
237.288054	120.228706	50.429287
233.344757	122.922037	50.434292
229.942984	121.572318	50.439297
225.960972	122.751797	50.444301
222.819000	124.454472	50.449306
219.911875	120.198617	50.454311
215.837163	129.825575	50.459316
212.519615	120.645883	50.464321
208.965180	126.159504	50.469325
205.486822	124.577196	50.474330
202.110904	124.220747	50.479335
198.338875	125.999723	50.484340
195.009958	129.449984	50.489345
191.367532	118.271614	50.494349
187.845981	124.180397	50.499354
184.886268	122.833308	50.504359
180.913487	129.208114	50.509364
177.570151	123.376562	50.514369
173.686891	123.187009	50.519373
170.517425	125.183369	50.524378
166.966272	116.188422	50.529383
163.070051	126.097267	50.534388
160.033339	122.854320	50.539393
156.842764	122.701459	50.544397
153.344037	121.640965	50.549402
149.693113	116.068946	50.554407
146.016189	118.690628	50.559412
142.369266	126.470808	50.564417
138.903738	125.733589	50.569421
134.875687	120.972314	50.574426
131.923594	117.469698	50.579431
128.162334	119.037974	50.584436
125.097903	118.161346	50.589441
121.380054	127.998463	50.594445
117.853943	120.329845	50.599450
114.736209	121.574517	50.604455
110.840878	129.713561	50.609460
107.294808	119.071067	50.614465
104.060571	122.357520	50.619469
100.239708	124.753642	50.624474
96.902178	116.693882	50.629479
93.488402	122.982127	50.634484
89.999529	122.393263	50.639489
86.696851	127.967515	50.644493
82.735474	124.063327	50.649498
79.121395	117.047492	50.654503
75.594275	122.467695	50.659508
72.471350	118.381670	50.664513
69.089398	120.642787	50.669517
65.234115	127.833161	50.674522
62.042255	114.129617	50.679527
58.314751	126.320214	50.684532
55.351057	119.106329	50.689537
51.499492	118.263001	50.694541
47.663827	116.779457	50.699546
44.527922	117.813279	50.704551
40.686277	118.922523	50.709556
37.159279	115.793809	50.714561
33.672764	115.312150	50.719565
30.228607	117.509201	50.724570
26.861984	114.752951	50.729575
23.009871	115.408299	50.734580
19.545507	111.826806	50.739585
16.147658	112.318730	50.744589
12.603770	109.692290	50.749594
9.796124	112.826276	50.754599
6.693281	122.311615	50.759604
2.451694	114.739680	50.764609