Tue Jun 21 12:27:22 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.992366	107.489079	0.000000
1.115897	108.461746	0.005005
1.096472	112.311938	0.010010
1.240602	108.911026	0.015014
1.258936	114.012775	0.020019
0.956857	98.870948	0.025024
1.019229	94.113684	0.030029
0.651628	87.200310	0.035034
0.425414	72.122316	0.040038
0.427906	69.599323	0.045043
-0.048766	49.047146	0.050048
-0.313556	40.025427	0.055053
-1.091324	33.864155	0.060058
-1.102874	25.143081	0.065062
-1.226980	18.286309	0.070067
-1.758364	11.633537	0.075072
-1.871677	5.035463	0.080077
-2.237185	10.933635	0.085082
-2.981636	1.906318	0.090086
-3.426502	10.486363	0.095091
-3.595010	-0.331418	0.100096
-3.598690	1.705016	0.105101
-3.999318	4.277033	0.110106
-3.838844	-2.171213	0.115110
-3.836965	7.735128	0.120115
-4.620687	1.995372	0.125120
-4.656674	1.549773	0.130125
-5.206418	14.425763	0.135130
-5.159857	1.996070	0.140134
-5.458545	8.888390	0.145139
-6.042853	4.818005	0.150144
-6.385100	9.987520	0.155149
-6.510221	8.187189	0.160154
-6.543922	5.556537	0.165158
-6.640037	9.324287	0.170163
-6.858845	9.872540	0.175168
-7.049197	6.920916	0.180173
-8.007258	5.000207	0.185178
-7.859298	4.728979	0.190182
-7.769882	10.422762	0.195187
-8.204353	4.550185	0.200192
-8.395221	9.089412	0.205197
-9.333804	14.085951	0.210202
-9.499854	11.372036	0.215206
-9.747176	10.088431	0.220211
-9.756539	11.153349	0.225216
-9.725700	0.819768	0.230221
-10.044108	7.574655	0.235226
-9.781253	-0.350218	0.240230
-10.196613	1.245269	0.245235
-11.345532	2.628738	0.250240
-11.320747	-0.767778	0.255245
-11.622470	6.586409	0.260250
-11.500994	0.118375	0.265254
-12.033058	-2.898218	0.270259
-11.743671	7.430361	0.275264
-11.814834	4.701128	0.280269
-12.870422	7.800346	0.285274
-13.060053	8.236221	0.290278
-13.044526	8.645227	0.295283
-13.565589	1.745072	0.300288
-13.222838	2.129687	0.305293
-14.215564	9.341771	0.310298
-14.383948	1.547508	0.315302
-14.965957	5.859453	0.320307
-15.142134	7.317851	0.325312
-14.832751	5.228699	0.330317
-15.041798	2.824417	0.335322
-15.071400	4.527112	0.340326
-14.889655	3.846940	0.345331
-15.739701	6.358997	0.350336
-15.968263	6.372119	0.355341
-16.512400	11.128108	0.360346
-16.261471	11.035780	0.365350
-16.684425	7.871667	0.370355
-17.658517	12.435219	0.375360
-17.596903	17.761437	0.380365
-17.969319	11.497927	0.385370
-17.849248	3.956830	0.390374
-18.393511	13.066600	0.395379
-18.240250	13.693543	0.400384
-18.362258	14.856049	0.405389
-18.522740	15.538105	0.410394
-18.932073	9.313467	0.415398
-19.403770	3.669452	0.420403
-19.554484	12.870339	0.425408
-19.398561	5.949244	0.430413
-20.137680	6.845718	0.435418
-20.883701	8.942134	0.440422
-20.922043	9.194892	0.445427
-21.037800	15.903003	0.450432
-21.138314	8.779088	0.455437
-21.373915	16.274670	0.460442
-21.112328	8.646989	0.465446
-21.712146	3.563700	0.470451
-22.188035	14.822353	0.475456
-22.087791	16.556235	0.480461
-22.308077	20.333895	0.485466
-22.672315	14.791664	0.490470
-23.147517	-0.539048	0.495475
-23.863686	11.606149	0.500480
-24.034966	5.019847	0.505485
-24.200627	11.960391	0.510490
-24.290515	-2.955397	0.515494
-24.327059	4.158134	0.520499
-24.453093	12.386818	0.525504
-23.946927	8.855921	0.530509
-25.262919	12.780494	0.535514
-25.458830	13.491111	0.540518
-25.693221	12.134917	0.545523
-25.963783	13.837852	0.550528
-25.601212	7.152686	0.555533
-26.861787	4.748490	0.560538
-27.115610	13.353732	0.565542
-27.150333	9.084200	0.570547
-27.407433	4.448935	0.575552
-27.276205	1.394135	0.580557
-27.469370	5.614851	0.585562
-27.549126	0.583179	0.590566
-27.579152	2.612333	0.595571
-28.477834	9.600067	0.600576
-28.640935	8.196943	0.605581
-29.173584	10.301637	0.610586
-28.921687	8.074398	0.615590
-29.494848	7.999350	0.620595
-30.472307	9.153151	0.625600
-30.128431	7.143139	0.630605
-30.327382	-1.266671	0.635610
-30.638302	8.255558	0.640614
-30.868289	5.348388	0.645619
-30.812264	14.663236	0.650624
-30.707377	17.019133	0.655629
-30.747965	10.457955	0.660634
-31.238611	6.425343	0.665638
-31.570386	8.261748	0.670643
-32.156661	12.100408	0.675648
-32.130411	7.118866	0.680653
-33.454723	14.162484	0.685658
-33.583666	11.157674	0.690662
-33.430036	11.205777	0.695667
-33.991414	11.826153	0.700672
-33.111424	13.902534	0.705677
-34.070389	10.382793	0.710682
-33.934877	5.941017	0.715686
-33.758625	10.040766	0.720691
-34.197970	13.890418	0.725696
-34.693551	12.240434	0.730701
-35.128729	6.268325	0.735706
-35.138432	8.808364	0.740710
-36.103732	15.543299	0.745715
-36.629387	10.280785	0.750720
-36.273824	11.305201	0.755725
-36.570224	6.827799	0.760730
-36.787776	10.005111	0.765734
-36.545951	11.524528	0.770739
-36.673984	5.546744	0.775744
-36.975532	0.887269	0.780749
-38.213062	19.269879	0.785754
-37.993815	10.917892	0.790758
-38.077777	6.199886	0.795763
-38.465035	12.912700	0.800768
-38.526963	4.193078	0.805773
-38.640124	15.289839	0.810778
-39.563215	7.608719	0.815782
-39.986494	13.968352	0.820787
-40.361016	14.485167	0.825792
-40.103109	1.530500	0.830797
-40.244778	5.678555	0.835802
-40.303323	3.013933	0.840806
-40.244964	9.426214	0.845811
-40.439676	18.565915	0.850816
-41.143457	8.219011	0.855821
-41.722955	10.783555	0.860826
-41.606347	3.674008	0.865830
-41.802325	6.430781	0.870835
-41.753794	15.596502	0.875840
-42.167702	10.321403	0.880845
-43.419748	12.110311	0.885850
-43.341224	10.323420	0.890854
-43.622751	6.646899	0.895859
-43.515781	10.944995	0.900864
-43.442450	7.126039	0.905869
-43.425812	11.275703	0.910874
-43.462140	0.181084	0.915878
-44.181932	8.683917	0.920883
-44.700882	9.588926	0.925888
-44.548098	0.682198	0.930893
-45.866457	8.436019	0.935898
-45.848152	5.589556	0.940902
-45.440208	4.188756	0.945907
-46.208068	6.647544	0.950912
-46.348198	5.278110	0.955917
-46.617502	12.790125	0.960922
-46.720172	2.570614	0.965926
-46.706744	2.640356	0.970931
-46.891149	12.144596	0.975936
-47.673303	10.082088	0.980941
-48.029439	9.275898	0.985946
-47.901223	6.291254	0.990950
-48.251224	7.048504	0.995955
-48.315507	7.013900	1.000960
-48.185858	6.647431	1.005965
-49.189610	13.950147	1.010970
-49.793992	14.977050	1.015974
-49.903719	4.912231	1.020979
-49.960105	-0.380434	1.025984
-49.648637	-1.891746	1.030989
-49.539155	9.452693	1.035994
-49.927700	7.296784	1.040998
-50.821844	5.353069	1.046003
-51.620203	12.861925	1.051008
-51.114042	5.703455	1.056013
-51.379042	4.789820	1.061018
-51.337370	13.803741	1.066022
-51.341726	2.495444	1.071027
-52.224228	8.153634	1.076032
-52.559844	5.333814	1.081037
-52.700128	11.230998	1.086042
-52.479515	-1.454050	1.091046
-53.642477	-1.350316	1.096051
-54.179795	6.990677	1.101056
-53.481566	6.136368	1.106061
-53.900027	12.274979	1.111066
-54.544815	11.953093	1.116070
-54.648655	4.791254	1.121075
-54.575581	19.237883	1.126080
-54.129092	14.014671	1.131085
-54.971538	8.506058	1.136090
-55.849785	2.955425	1.141094
-55.722698	8.377156	1.146099
-55.998435	11.927000	1.151104
-56.073489	2.349577	1.156109
-56.377660	8.742764	1.161114
-56.932816	9.314358	1.166118
-56.964041	11.570842	1.171123
-57.680951	12.918694	1.176128
-57.501150	4.895883	1.181133
-57.598790	14.849290	1.186138
-57.766162	7.504980	1.191142
-57.848547	2.328508	1.196147
-58.781980	8.882343	1.201152
-58.912641	2.442647	1.206157
-58.994558	6.777942	1.211162
-59.196353	7.521305	1.216166
-58.826622	9.040257	1.221171
-59.807273	9.861100	1.226176
-59.938727	9.414341	1.231181
-60.413262	10.161432	1.236186
-60.499322	1.932828	1.241190
-60.538531	6.388527	1.246195
-60.918395	16.666124	1.251200
-61.259493	3.016589	1.256205
-61.897902	7.762934	1.261210
-62.306792	10.928520	1.266214
-62.187798	6.571177	1.271219
-62.394234	13.074472	1.276224
-61.904663	0.665746	1.281229
-62.220962	10.122365	1.286234
-62.754660	15.254720	1.291238
-63.349779	18.605463	1.296243
-63.819644	13.249650	1.301248
-63.663233	10.638426	1.306253
-64.082346	12.374252	1.311258
-64.292181	6.786727	1.316262
-64.236157	4.907659	1.321267
-65.359552	14.162674	1.326272
-65.325680	1.138157	1.331277
-65.265183	5.893669	1.336282
-65.576302	7.510575	1.341286
-65.660477	10.800183	1.346291
-65.755737	2.785038	1.351296
-65.639111	2.968719	1.356301
-66.609279	6.488132	1.361306
-67.031626	9.301734	1.366310
-67.038042	4.309817	1.371315
-67.282902	6.769807	1.376320
-67.071517	7.080664	1.381325
-67.432155	-0.253933	1.386330
-68.227001	12.588449	1.391334
-68.253938	8.032681	1.396339
-68.961950	19.283406	1.401344
-68.752592	9.889561	1.406349
-69.047628	10.140628	1.411354
-69.010663	17.975475	1.416358
-69.397145	8.930329	1.421363
-70.040507	13.244154	1.426368
-70.306664	6.784470	1.431373
-70.357175	10.484875	1.436378
-70.573694	10.884949	1.441382
-70.307502	7.663349	1.446387
-70.503583	13.820387	1.451392
-71.156460	7.010546	1.456397
-71.624704	13.921477	1.461402
-72.023826	7.751003	1.466406
-72.028366	5.345416	1.471411
-72.299306	3.583051	1.476416
-72.230853	-1.166703	1.481421
-72.940454	14.114609	1.486426
-73.187491	11.264531	1.491430
-73.314714	13.044172	1.496435
-73.352705	5.760331	1.501440
-73.393427	14.746456	1.506445
-73.448750	11.688410	1.511450
-74.310645	6.736938	1.516454
-74.493816	7.390193	1.521459
-75.022667	4.918111	1.526464
-74.717587	1.200093	1.531469
-75.059836	7.860065	1.536474
-76.001332	8.252530	1.541478
-76.355645	7.010724	1.546483
-76.858928	12.748393	1.551488
-75.999303	7.980680	1.556493
-76.356073	10.141696	1.561498
-76.368703	7.859795	1.566502
-76.283819	9.186357	1.571507
-77.585575	13.554560	1.576512
-78.006409	6.456073	1.581517
-77.990383	17.594584	1.586522
-78.299464	9.133948	1.591526
-77.783880	2.905526	1.596531
-78.298289	16.247291	1.601536
-78.606112	8.116783	1.606541
-79.426043	14.023715	1.611546
-79.661471	10.840591	1.616550
-79.582110	8.400586	1.621555
-80.037870	16.867987	1.626560
-79.687978	11.655443	1.631565
-79.630958	11.451961	1.636570
-80.411606	15.643287	1.641574
-80.905104	3.379607	1.646579
-81.440720	10.869422	1.651584
-81.041566	8.605954	1.656589
-81.381001	7.190794	1.661594
-81.578377	5.748752	1.666598
-81.571849	13.396040	1.671603
-82.809059	11.032194	1.676608
-82.945550	3.876752	1.681613
-83.201416	8.359058	1.686618
-83.241919	2.010401	1.691622
-82.998437	11.454430	1.696627
-83.591338	8.360109	1.701632
-83.096370	6.841492	1.706637
-83.621775	7.171362	1.711642
-84.412169	6.359543	1.716646
-84.699636	2.847797	1.721651
-84.634537	10.197671	1.726656
-84.818822	1.380709	1.731661
-85.770813	9.137011	1.736666
-86.132539	4.790215	1.741670
-85.934049	3.209995	1.746675
-86.271761	14.523513	1.751680
-86.140824	5.775703	1.756685
-86.295026	2.469412	1.761690
-86.429800	14.749207	1.766694
-86.658868	-2.525330	1.771699
-87.437374	10.602058	1.776704
-87.745702	-0.568670	1.781709
-88.061834	2.641149	1.786714
-87.920359	5.703353	1.791718
-87.803400	3.124317	1.796723
-88.654189	7.320944	1.801728
-89.262089	4.631667	1.806733
-89.615245	5.511395	1.811738
-89.714615	11.088831	1.816742
-89.719038	-0.433752	1.821747
-89.660282	0.240610	1.826752
-89.338672	5.281434	1.831757
-89.552077	1.321318	1.836762
-90.477559	11.099050	1.841766
-91.257966	2.867044	1.846771
-91.084300	1.532667	1.851776
-91.314432	-1.347635	1.856781
-91.246258	-5.365434	1.861786
-91.941442	7.028873	1.866790
-92.161461	4.154394	1.871795
-92.855445	12.502788	1.876800
-92.776500	3.019645	1.881805
-92.749686	12.177510	1.886810
-92.934293	7.373957	1.891814
-92.904890	7.180969	1.896819
-93.699711	8.353475	1.901824
-94.110868	-0.893392	1.906829
-94.369221	0.358393	1.911834
-94.336497	10.139836	1.916838
-94.587938	8.902898	1.921843
-94.944234	13.279491	1.926848
-95.007056	6.907101	1.931853
-94.812148	5.629984	1.936858
-95.198566	8.712720	1.941862
-95.405340	-1.133750	1.946867
-96.325564	-0.550431	1.951872
-96.206937	-1.194696	1.956877
-96.813140	8.274808	1.961882
-97.569630	8.549417	1.966886
-96.963674	1.318376	1.971891
-97.310949	13.425965	1.976896
-97.738268	4.096327	1.981901
-98.000716	3.897407	1.986906
-98.051017	3.460100	1.991910
-97.933040	5.714565	1.996915
-98.302017	5.088322	2.006912
-98.534704	6.574052	2.016909
-97.832189	9.220223	2.026906
-97.555142	5.952980	2.036902
-96.598546	13.657153	2.046899
-96.686712	8.121452	2.056896
-95.687440	9.356914	2.066893
-95.287496	6.907475	2.076890
-95.131802	7.526488	2.086886
-94.172948	4.475899	2.096883
-93.876093	14.364578	2.106880
-93.282699	19.649997	2.116877
-92.315462	15.104863	2.126874
-92.141473	7.509383	2.136870
-92.220734	5.742735	2.146867
-91.267814	10.429199	2.156864
-90.863545	13.591465	2.166861
-90.290026	9.683352	2.176858
-89.524513	10.603258	2.186854
-89.242252	8.407844	2.196851
-88.987986	4.190629	2.206848
-88.165477	13.394555	2.216845
-87.654525	3.911059	2.226842
-87.496388	7.552924	2.236838
-86.681156	12.448122	2.246835
-86.463935	12.253166	2.256832
-85.822851	16.294986	2.266829
-84.928810	14.654236	2.276826
-84.691979	9.047916	2.286822
-84.528481	10.326758	2.296819
-84.082382	14.715624	2.306816
-82.949653	14.637765	2.316813
-83.246064	20.244820	2.326810
-82.118274	14.550614	2.336806
-81.508750	14.322499	2.346803
-81.377476	7.840179	2.356800
-80.439957	13.255324	2.366797
-79.985953	10.799897	2.376794
-79.743460	11.012130	2.386790
-79.799564	8.678724	2.396787
-78.882593	12.948510	2.406784
-78.379668	9.913563	2.416781
-77.233137	11.043039	2.426778
-77.099428	13.025281	2.436774
-77.125729	9.975828	2.446771
-76.304141	17.147942	2.456768
-75.405129	16.364881	2.466765
-75.169385	15.622707	2.476762
-74.862918	12.276892	2.486758
-74.231312	7.086709	2.496755
-74.092026	10.854201	2.506752
-73.126672	14.762891	2.516749
-72.844096	13.408942	2.526746
-72.227915	13.376917	2.536742
-71.359804	13.403346	2.546739
-70.910105	15.268843	2.556736
-70.805661	10.441793	2.566733
-70.712050	8.597711	2.576730
-69.775059	5.630968	2.586726
-69.292552	7.353117	2.596723
-68.684568	9.528889	2.606720
-68.019242	11.476437	2.616717
-67.509288	6.152681	2.626714
-67.718596	10.199990	2.636710
-66.527714	11.067831	2.646707
-66.228315	9.501261	2.656704
-65.675512	5.451356	2.666701
-64.798245	12.120088	2.676698
-64.376880	10.578764	2.686694
-64.776782	16.263616	2.696691
-63.944018	10.429777	2.706688
-63.054163	13.387940	2.716685
-62.923068	11.672996	2.726682
-61.924744	10.490174	2.736678
-61.417213	6.946473	2.746675
-61.369767	9.507503	2.756672
-61.104496	10.102048	2.766669
-60.077926	5.469050	2.776666
-59.799219	20.242889	2.786662
-58.859332	12.978570	2.796659
-58.550325	6.468593	2.806656
-58.341490	12.957772	2.816653
-57.846637	13.290629	2.826650
-56.990152	11.218452	2.836646
-56.688660	13.541999	2.846643
-56.256327	14.598494	2.856640
-55.587927	11.642446	2.866637
-55.149630	13.579779	2.876634
-55.038358	14.089179	2.886630
-53.849778	11.544112	2.896627
-53.372023	19.896252	2.906624
-53.360393	15.970940	2.916621
-53.104604	8.887095	2.926618
-52.201172	3.510428	2.936614
-51.675894	12.455355	2.946611
-50.566132	14.886695	2.956608
-50.399577	16.059522	2.966605
-50.486961	14.098409	2.976602
-50.104734	11.471511	2.986598
-49.147990	12.964764	2.996595
-48.838223	18.120322	3.006592
-47.618459	17.001008	3.016589
-47.771307	15.091043	3.026586
-47.297507	20.188218	3.036582
-46.811983	16.798327	3.046579
-46.144275	15.906375	3.056576
-45.778815	19.511937	3.066573
-45.081326	16.994849	3.076570
-44.311586	15.977329	3.086566
-44.586914	19.918405	3.096563
-43.580184	20.553961	3.106560
-43.126304	20.352813	3.116557
-42.850249	16.803778	3.126554
-42.161492	17.302112	3.136550
-41.197653	14.827855	3.146547
-41.072951	16.108580	3.156544
-41.097802	7.336604	3.166541
-39.894261	9.134961	3.176538
-39.717662	12.055945	3.186534
-39.277321	17.034183	3.196531
-38.208801	12.040561	3.206528
-37.866759	16.296305	3.216525
-37.701952	13.100009	3.226522
-37.604231	14.651351	3.236518
-36.465720	17.476663	3.246515
-36.408176	14.661688	3.256512
-35.590296	15.599410	3.266509
-34.599769	11.443231	3.276506
-34.524813	16.467554	3.286502
-34.487333	14.311887	3.296499
-33.764922	15.359470	3.306496
-33.210799	14.586506	3.316493
-32.815415	16.389675	3.326490
-31.683315	16.185677	3.336486
-31.568734	16.501686	3.346483
-31.539628	22.555913	3.356480
-30.666335	16.967089	3.366477
-29.989020	12.169451	3.376474
-29.762971	10.539749	3.386470
-28.651518	12.866095	3.396467
-28.200891	18.614402	3.406464
-28.096375	17.552928	3.416461
-27.989156	13.036022	3.426458
-27.156833	7.184084	3.436454
-26.754828	13.689093	3.446451
-25.986624	11.607633	3.456448
-25.230404	7.859744	3.466445
-24.992809	19.129694	3.476442
-24.893777	7.191042	3.486438
-24.432657	10.488534	3.496435
-23.767892	15.468929	3.506432
-23.088463	15.505274	3.516429
-22.192176	8.724167	3.526426
-22.257142	3.155575	3.536422
-21.754734	6.274330	3.546419
-20.915579	10.905756	3.556416
-20.405198	9.306028	3.566413
-20.216290	3.841410	3.576410
-19.808072	15.030151	3.586406
-19.078029	7.807901	3.596403
-18.643042	10.426074	3.606400
-18.231681	4.064726	3.616397
-17.599795	7.723578	3.626394
-17.213864	9.832398	3.636390
-16.302165	8.532142	3.646387
-15.747573	15.130437	3.656384
-15.615691	8.118680	3.666381
-15.727615	12.286593	3.676378
-14.606958	4.005606	3.686374
-13.931010	4.893333	3.696371
-13.051863	10.081455	3.706368
-12.923745	12.295011	3.716365
-12.602855	10.614632	3.726362
-12.229752	8.506329	3.736358
-11.907593	8.103923	3.746355
-10.746962	12.539657	3.756352
-10.793330	13.011540	3.766349
-9.683024	12.785470	3.776346
-9.305937	12.968504	3.786342
-9.373155	11.125566	3.796339
-8.925051	17.575130	3.806336
-8.115311	14.095197	3.816333
-7.539798	10.146849	3.826330
-6.521664	8.869672	3.836326
-6.041989	15.475831	3.846323
-5.920380	10.286528	3.856320
-5.992446	12.587965	3.866317
-5.603934	11.784536	3.876314
-4.616454	7.072863	3.886310
-3.955138	13.558053	3.896307
-3.407809	17.148321	3.906304
-3.165297	24.214813	3.916301
-2.865473	24.091342	3.926298
-2.237770	34.495892	3.936294
-2.444154	41.348843	3.946291
-1.241255	61.489463	3.956288
-1.101165	75.004775	3.966285
-0.402078	92.415625	3.976282
-0.026748	103.928786	3.986278
0.000000	114.548184	3.991283
0.765415	114.462223	3.996288
0.333056	131.874143	4.001293
0.996457	142.597315	4.006298
1.029274	148.117000	4.011302
1.164783	147.554789	4.016307
1.229979	158.005252	4.021312
1.271963	160.499067	4.026317
1.278672	152.865174	4.031322
1.162671	162.476187	4.036326
0.934754	154.770243	4.041331
1.207669	148.237405	4.046336
1.069394	155.179596	4.051341
1.448509	154.500677	4.056346
1.039765	162.006255	4.061350
0.989990	161.045719	4.066355
1.262697	153.870193	4.071360
1.080808	165.556243	4.076365
1.448641	159.608765	4.081370
1.365639	165.863370	4.086374
1.128545	165.352992	4.091379
1.442280	159.908205	4.096384
1.015676	161.888794	4.101389
1.818274	174.795737	4.106394
1.318389	177.591618	4.111398
1.151988	173.796531	4.116403
1.568628	171.849833	4.121408
1.482321	196.210712	4.126413
1.879599	179.194541	4.131418
1.757974	173.366787	4.136422
1.558167	171.947426	4.141427
1.547149	164.336591	4.146432
1.420168	165.026918	4.151437
1.505912	160.318254	4.156442
1.381548	164.072171	4.161446
1.457660	164.372677	4.166451
1.475804	165.610653	4.171456
1.639523	168.627772	4.176461
1.644331	169.304762	4.181466
1.484551	166.979122	4.186470
1.608233	175.390517	4.191475
1.808584	179.770684	4.196480
1.488034	180.156412	4.201485
1.648723	182.653661	4.206490
1.790660	182.894329	4.211494
1.736238	180.987747	4.216499
1.686199	170.842283	4.221504
1.797501	182.358829	4.226509
1.894554	180.961744	4.231514
1.454702	172.663557	4.236518
1.830588	179.434776	4.241523
2.058217	184.655022	4.246528
1.386095	176.227166	4.251533
1.643453	178.252168	4.256538
1.962158	184.127484	4.261542
1.831924	185.592892	4.266547
1.916297	184.879306	4.271552
1.843024	194.283758	4.276557
1.893545	184.161495	4.281562
1.994271	194.130915	4.286566
1.820327	187.067422	4.291571
2.066644	176.431441	4.296576
1.830725	178.291852	4.301581
1.790872	172.840097	4.306586
1.745244	174.860807	4.311590
1.646358	193.042830	4.316595
1.776631	183.162911	4.321600
1.583900	194.661731	4.326605
1.833339	182.170670	4.331610
1.917204	186.699580	4.336614
1.986736	191.858786	4.341619
2.134638	190.409867	4.346624
1.784009	198.032923	4.351629
1.772197	191.945241	4.356634
2.160416	190.892441	4.361638
1.925206	198.705757	4.366643
2.078099	196.083838	4.371648
1.765788	202.196064	4.376653
2.163138	191.142365	4.381658
1.876249	193.237759	4.386662
2.017029	198.106729	4.391667
1.981276	196.985606	4.396672
2.345054	208.046944	4.401677
2.492621	209.022940	4.406682
2.468646	198.361450	4.411686
2.023476	194.605614	4.416691
1.944480	189.678538	4.421696
2.027677	203.205471	4.426701
2.214640	195.924144	4.431706
2.230406	207.792986	4.436710
2.416071	213.979243	4.441715
2.259837	199.250463	4.446720
2.040768	206.568955	4.451725
2.085495	216.087082	4.456730
2.346222	220.996384	4.461734
2.534482	227.404811	4.466739
2.306538	215.263914	4.471744
2.341367	228.278898	4.476749
2.449756	222.804749	4.481754
2.591270	222.728961	4.486758
2.474630	216.056360	4.491763
2.643956	206.426890	4.496768
2.262834	195.078616	4.501773
2.167421	198.732236	4.506778
2.271762	199.072272	4.511782
2.573264	223.985255	4.516787
2.482524	218.003381	4.521792
2.153287	227.397748	4.526797
2.372749	220.073139	4.531802
2.511545	228.269333	4.536806
2.403364	226.031045	4.541811
2.717329	222.477663	4.546816
2.515440	225.807925	4.551821
2.397042	227.548832	4.556826
2.551965	221.852473	4.561830
2.442570	228.161991	4.566835
2.613551	229.123257	4.571840
2.465536	237.721759	4.576845
2.302661	221.554294	4.581850
2.621265	224.389485	4.586854
2.480017	226.888394	4.591859
2.717548	227.010223	4.596864
2.491352	232.028577	4.601869
2.559980	226.418533	4.606874
2.546221	231.906494	4.611878
2.626743	222.970950	4.616883
3.044710	217.100990	4.621888
2.627752	230.976186	4.626893
2.483359	228.336987	4.631898
2.634495	225.183928	4.636902
2.518455	234.852220	4.641907
2.595040	224.854080	4.646912
2.910522	219.960537	4.651917
2.767782	227.915241	4.656922
2.798600	230.713629	4.661926
2.886182	227.374547	4.666931
2.910518	221.786048	4.671936
2.861108	228.257512	4.676941
2.898157	227.686542	4.681946
2.943187	221.730728	4.686950
2.774931	228.091829	4.691955
2.914940	220.073125	4.696960
2.905939	226.658273	4.701965
2.942319	224.225351	4.706970
2.765587	227.456134	4.711974
2.978360	230.267806	4.716979
3.106656	231.051829	4.721984
2.530176	231.371206	4.726989
2.861853	227.496587	4.731994
3.285394	241.615246	4.736998
2.919362	243.502144	4.742003
3.024799	234.195028	4.747008
3.006717	248.467928	4.752013
3.043341	248.859633	4.757018
3.109035	245.459248	4.762022
2.531178	245.308996	4.767027
3.280968	248.468647	4.772032
2.931984	263.181161	4.777037
3.057181	257.159371	4.782042
3.258762	261.594611	4.787046
3.208651	264.018049	4.792051
3.313789	253.245945	4.797056
3.210266	258.007782	4.802061
3.269709	252.258155	4.807066
3.185283	253.959892	4.812070
2.980938	256.538321	4.817075
3.340956	253.812039	4.822080
3.228750	257.672499	4.827085
3.045113	255.070776	4.832090
3.452181	253.257474	4.837094
3.282512	259.522916	4.842099
3.145387	254.176239	4.847104
3.054216	258.751126	4.852109
2.956627	255.159720	4.857114
3.061016	262.135776	4.862118
2.965940	256.014497	4.867123
3.203752	251.558671	4.872128
3.074759	268.713502	4.877133
2.941971	255.837920	4.882138
3.253631	248.749832	4.887142
2.976489	268.341236	4.892147
3.402286	269.137763	4.897152
3.361383	288.917997	4.902157
3.684142	288.655510	4.907162
3.695177	282.134408	4.912166
3.373392	281.510966	4.917171
3.483183	267.524258	4.922176
3.456004	270.023624	4.927181
3.522311	272.722408	4.932186
3.488246	258.180545	4.937190
3.229042	256.663266	4.942195
3.839762	263.520944	4.947200
3.732058	280.047101	4.952205
3.248204	271.643073	4.957210
3.467221	278.413080	4.962214
3.441023	276.551935	4.967219
3.952024	273.166408	4.972224
3.555473	280.718568	4.977229
3.837361	274.653853	4.982234
3.563027	250.056445	4.987238
3.359927	263.844555	4.992243
3.663860	277.730660	4.997248
3.945723	276.495762	5.002253
3.966059	266.106317	5.007258
3.405336	267.465022	5.012262
3.238916	262.099118	5.017267
3.807947	276.853018	5.022272
3.931575	276.724740	5.027277
3.671602	287.870678	5.032282
3.753118	276.471782	5.037286
3.719242	292.313795	5.042291
3.821930	287.490989	5.047296
3.356667	291.491619	5.052301
3.622831	289.443727	5.057306
3.817094	291.549641	5.062310
3.558975	279.123014	5.067315
3.871189	277.266610	5.072320
3.867450	281.629294	5.077325
3.754384	287.749409	5.082330
4.038340	282.705763	5.087334
3.909493	292.929347	5.092339
3.920793	289.202289	5.097344
4.036254	291.223769	5.102349
3.877826	289.081409	5.107354
3.645182	289.170392	5.112358
3.666969	288.082161	5.117363
3.921363	280.227416	5.122368
4.089205	289.142071	5.127373
4.178052	291.874028	5.132378
4.308100	281.378393	5.137382
4.024533	289.297839	5.142387
4.511552	277.845804	5.147392
4.025659	284.347143	5.152397
4.083678	290.020378	5.157402
4.366107	281.859262	5.162406
3.998513	288.345157	5.167411
4.084499	281.355204	5.172416
4.238218	292.819618	5.177421
4.240769	288.290060	5.182426
4.092263	277.184607	5.187430
3.934838	287.260576	5.192435
4.330827	280.511742	5.197440
4.128638	292.601250	5.202445
4.105804	291.073440	5.207450
4.309358	282.297855	5.212454
3.960185	283.236131	5.217459
3.992549	281.775946	5.222464
3.849011	292.215677	5.227469
4.148267	292.103506	5.232474
4.084878	286.849985	5.237478
3.553534	290.657117	5.242483
3.825800	287.990353	5.247488
4.069267	293.816600	5.252493
4.576953	294.499716	5.257498
4.305134	285.895003	5.262502
4.024715	295.434065	5.267507
4.236108	293.311176	5.272512
4.568671	312.061265	5.277517
4.252742	302.561820	5.282522
4.113344	299.700370	5.287526
4.012928	318.921575	5.292531
4.353605	311.319129	5.297536
4.402589	312.152600	5.302541
4.464975	318.876731	5.307546
4.139566	317.671348	5.312550
4.081732	328.920794	5.317555
4.485566	313.799998	5.322560
4.399336	314.402281	5.327565
4.345722	326.604757	5.332570
4.594274	315.781629	5.337574
4.258758	316.473146	5.342579
4.211175	316.342829	5.347584
4.387694	314.666168	5.352589
4.641810	317.138300	5.357594
4.715172	319.052298	5.362598
4.342730	317.867136	5.367603
4.764003	314.662617	5.372608
4.751832	310.075696	5.377613
4.483531	311.157663	5.382618
4.499000	312.613756	5.387622
4.508061	327.932463	5.392627
4.865171	309.809029	5.397632
4.842103	310.552210	5.402637
4.502430	315.944193	5.407642
4.636257	311.224561	5.412646
4.366310	320.869848	5.417651
4.561571	309.006111	5.422656
4.545652	328.948417	5.427661
4.650480	343.885812	5.432666
4.963855	348.260533	5.437670
4.703205	354.681385	5.442675
4.940425	341.860100	5.447680
4.865863	351.938176	5.452685
4.685069	346.623365	5.457690
4.838831	336.938177	5.462694
4.570332	350.779029	5.467699
4.913210	343.038068	5.472704
4.767483	352.640307	5.477709
4.768070	358.434573	5.482714
4.724884	344.933318	5.487718
4.519237	347.883762	5.492723
4.707754	347.197916	5.497728
4.823369	350.584756	5.502733
4.934823	345.899603	5.507738
5.030239	348.582727	5.512742
4.635151	342.412424	5.517747
4.770649	343.787273	5.522752
4.863229	346.933030	5.527757
4.776339	341.825268	5.532762
4.952168	351.418266	5.537766
4.864289	352.920485	5.542771
4.837404	349.223812	5.547776
4.952482	351.507426	5.552781
4.919723	364.060107	5.557786
5.095854	358.818404	5.562790
4.977843	370.832465	5.567795
5.323407	378.831498	5.572800
5.555677	373.831902	5.577805
4.754143	364.028615	5.582810
5.035178	357.022511	5.587814
5.141979	370.889049	5.592819
5.240010	360.025497	5.597824
5.415662	370.527276	5.602829
5.019472	353.885032	5.607834
5.312715	350.746897	5.612838
5.118316	360.934611	5.617843
4.896850	351.752401	5.622848
5.097759	370.946270	5.627853
5.108182	374.937417	5.632858
5.652269	373.504771	5.637862
5.335622	381.703448	5.642867
5.217902	372.510954	5.647872
5.286257	380.095305	5.652877
5.448451	381.275502	5.657882
5.203449	366.860031	5.662886
5.059128	384.873778	5.667891
5.185826	380.734492	5.672896
5.307289	376.857547	5.677901
5.354073	384.219521	5.682906
5.553586	375.499017	5.687910
5.344005	379.297881	5.692915
5.605484	375.727502	5.697920
5.224385	379.668041	5.702925
5.090891	376.167013	5.707930
5.214413	375.240126	5.712934
5.090532	390.398568	5.717939
5.154458	388.719034	5.722944
5.317780	390.746613	5.727949
5.132714	390.307928	5.732954
5.230359	378.751573	5.737958
5.061660	396.642482	5.742963
5.555659	400.177234	5.747968
5.367991	418.055127	5.752973
5.560501	420.904131	5.757978
5.477672	409.962944	5.762982
5.678722	409.776457	5.767987
5.999403	407.556718	5.772992
5.875318	408.646581	5.777997
5.567182	395.324728	5.783002
5.827492	387.775021	5.788006
5.554682	382.905631	5.793011
5.440862	384.097790	5.798016
5.655369	390.676188	5.803021
5.391489	410.294979	5.808026
5.618168	408.336689	5.813030
5.509073	413.869707	5.818035
5.722217	419.638664	5.823040
5.661745	424.021834	5.828045
5.473954	419.404959	5.833050
5.736067	419.985281	5.838054
5.655558	427.572204	5.843059
5.626936	420.437179	5.848064
5.401339	418.470702	5.853069
5.335223	415.751019	5.858074
5.981589	412.700427	5.863078
5.393392	419.255862	5.868083
5.784633	416.832032	5.873088
5.930912	419.443400	5.878093
5.974717	429.402072	5.883098
5.697119	418.688891	5.888102
5.887360	411.559068	5.893107
5.911536	412.601489	5.898112
6.078203	415.951868	5.903117
5.725313	424.112957	5.908122
5.989595	415.977471	5.913126
5.714297	430.531714	5.918131
5.935094	434.291293	5.923136
6.088322	440.111423	5.928141
6.198154	441.080263	5.933146
6.410715	424.732013	5.938150
6.178381	430.736560	5.943155
5.953385	415.079235	5.948160
6.097714	413.937550	5.953165
6.205864	411.065280	5.958170
6.097035	405.332212	5.963174
5.979340	417.506890	5.968179
5.980226	411.667048	5.973184
5.926337	417.576129	5.978189
5.771611	423.561113	5.983194
6.205193	414.170936	5.988198
6.047804	431.536276	5.993203
6.178313	439.513922	5.998208
6.655594	441.547140	6.003213
6.435849	427.837257	6.008218
6.106193	420.282218	6.013222
5.834910	424.600641	6.018227
5.889555	414.301716	6.023232
5.856195	420.414605	6.028237
6.216713	435.470382	6.033242
6.329268	433.910666	6.038246
6.143217	423.461161	6.043251
5.972074	419.495706	6.048256
5.983439	415.669544	6.053261
5.913721	431.185514	6.058266
6.136239	434.254321	6.063270
6.248517	451.004917	6.068275
6.643849	440.787302	6.073280
6.259337	431.366624	6.078285
5.984904	433.747904	6.083290
6.289344	417.480748	6.088294
5.861649	422.373869	6.093299
6.339498	424.183801	6.098304
6.155776	420.109327	6.103309
5.741513	428.294198	6.108314
6.125659	417.132411	6.113318
5.861185	423.592998	6.118323
5.912644	437.927967	6.123328
6.327397	442.371967	6.128333
5.912135	453.026118	6.133338
6.290610	441.831901	6.138342
6.235336	448.561758	6.143347
6.498012	444.137873	6.148352
6.131190	425.806798	6.153357
5.907612	423.017282	6.158362
6.444747	423.814128	6.163366
5.997149	417.970205	6.168371
5.784065	420.367176	6.173376
6.430751	431.528055	6.178381
5.919286	440.986668	6.183386
6.215093	435.882203	6.188390
6.138106	434.617716	6.193395
6.094503	439.639052	6.198400
6.086969	445.278205	6.203405
6.075608	447.133629	6.208410
5.853198	445.768109	6.213414
5.747868	452.945533	6.218419
6.164404	445.740728	6.223424
6.181606	450.003493	6.228429
6.066523	451.510819	6.233434
6.390948	446.814050	6.238438
6.199232	446.863496	6.243443
6.194646	445.482232	6.248448
6.359166	443.778536	6.253453
6.151153	442.962786	6.258458
6.235578	435.783775	6.263462
5.900840	453.181467	6.268467
6.145845	447.737502	6.273472
6.393997	449.344326	6.278477
5.804173	451.975568	6.283482
6.298406	448.769005	6.288486
6.205132	441.831752	6.293491
6.162986	454.229373	6.298496
6.344724	450.398276	6.303501
5.926232	435.917339	6.308506
6.379026	439.907869	6.313510
5.944773	437.485555	6.318515
5.917754	439.103212	6.323520
6.276657	442.229161	6.328525
6.276223	445.417771	6.333530
6.187574	435.307536	6.338534
5.881215	443.251160	6.343539
6.201929	450.886111	6.348544
6.169836	447.732169	6.353549
6.334431	442.720472	6.358554
5.964915	418.567374	6.363558
6.143478	427.533220	6.368563
6.141440	443.375839	6.373568
6.043269	442.580578	6.378573
5.957578	454.184412	6.383578
6.344107	439.412888	6.388582
6.158435	458.420260	6.393587
6.179904	455.577333	6.398592
6.330810	450.540273	6.403597
5.796884	440.678611	6.408602
6.167672	436.338257	6.413606
6.387628	454.471736	6.418611
5.975817	443.285442	6.423616
6.354090	434.952083	6.428621
5.979510	437.640035	6.433626
6.219736	422.183913	6.438630
6.053885	430.967816	6.443635
6.083120	427.859767	6.448640
6.289841	426.109617	6.453645
6.222654	431.402052	6.458650
6.321300	420.566576	6.463654
5.917708	428.555499	6.468659
6.058367	430.737010	6.473664
6.112604	419.778052	6.478669
5.913195	429.249710	6.483674
5.943465	432.240828	6.488678
6.454498	455.653855	6.493683
6.202157	443.092935	6.498688
6.055575	433.861374	6.503693
5.961232	435.892749	6.508698
6.174012	448.922853	6.513702
6.321704	441.088065	6.518707
5.872578	429.573668	6.523712
6.022689	441.714082	6.528717
6.168030	455.650684	6.533722
6.433697	448.612747	6.538726
6.075818	446.760723	6.543731
5.903003	450.121739	6.548736
6.098621	431.968664	6.553741
6.051897	454.177929	6.558746
6.085780	449.140316	6.563750
6.167050	456.644025	6.568755
6.253527	451.787148	6.573760
6.132565	450.381345	6.578765
5.857214	455.112691	6.583770
6.169561	450.504552	6.588774
6.240819	448.579493	6.593779
6.213657	454.247948	6.598784
6.519319	454.977550	6.603789
6.194179	446.331058	6.608794
6.253187	428.463267	6.613798
6.125231	427.430804	6.618803
5.996130	425.578788	6.623808
6.497368	422.940786	6.628813
5.904291	427.305195	6.633818
6.261518	421.148420	6.638822
6.062372	431.818472	6.643827
5.903394	431.146356	6.648832
5.836715	430.876919	6.653837
6.204070	442.599905	6.658842
6.474319	446.509366	6.663846
6.393111	437.902803	6.668851
6.161187	432.104661	6.673856
6.201047	431.427049	6.678861
6.060173	432.715849	6.683866
5.906634	421.566922	6.688870
5.598944	429.932669	6.693875
6.128074	437.744254	6.698880
6.402907	440.778547	6.703885
5.922341	444.633351	6.708890
6.128690	443.126777	6.713894
6.570657	452.342462	6.718899
6.308787	436.327724	6.723904
6.195087	434.460921	6.728909
5.788096	428.750577	6.733914
5.980949	427.248016	6.738918
6.063094	431.190398	6.743923
5.848986	427.789931	6.748928
6.288826	433.517013	6.753933
6.202279	454.405772	6.758938
6.200366	447.694536	6.763942
6.007678	445.065271	6.768947
5.986548	448.302301	6.773952
6.588090	449.593869	6.778957
5.977314	444.993353	6.783962
6.033052	431.120827	6.788966
6.030455	440.781908	6.793971
6.003729	447.705165	6.798976
6.275922	445.793404	6.803981
6.376632	453.874858	6.808986
6.205797	427.718024	6.813990
6.139052	432.660111	6.818995
6.288468	430.200545	6.824000
6.102615	426.799347	6.829005
5.906843	428.842387	6.834010
5.880479	422.119424	6.839014
6.334899	448.886110	6.844019
6.018089	449.661954	6.849024
5.978365	446.888759	6.854029
5.836271	451.624480	6.859034
6.092978	455.604663	6.864038
6.201891	456.368226	6.869043
6.345690	460.182398	6.874048
6.213704	450.560047	6.879053
6.351338	460.839467	6.884058
6.601504	447.895574	6.889062
6.247898	438.611463	6.894067
6.171170	427.050794	6.899072
6.295518	419.762760	6.904077
6.123030	426.461893	6.909082
6.198956	418.741813	6.914086
6.465496	423.477744	6.919091
6.255571	423.003510	6.924096
6.322011	424.226010	6.929101
6.182993	422.383135	6.934106
6.199228	419.803542	6.939110
6.241202	421.354517	6.944115
5.853150	425.926715	6.949120
6.233782	417.213690	6.954125
5.945526	425.842623	6.959130
6.049004	419.825945	6.964134
6.070842	420.258781	6.969139
6.330689	421.716845	6.974144
6.287514	413.311203	6.979149
6.050751	426.345279	6.984154
6.081349	411.587924	6.989158
6.073367	410.558487	6.994163
5.954264	415.600804	6.999168
6.294089	409.294570	7.004173
6.058665	420.620654	7.009178
6.289727	414.577720	7.014182
6.139713	420.450426	7.019187
6.326722	417.577923	7.024192
6.519693	420.368044	7.029197
6.078285	421.439807	7.034202
6.266702	420.267733	7.039206
6.022920	413.587684	7.044211
5.927318	423.914976	7.049216
6.021080	409.937110	7.054221
5.822532	420.340056	7.059226
5.989814	418.603740	7.064230
6.214928	419.974411	7.069235
5.972790	425.819157	7.074240
6.151289	413.796693	7.079245
6.007245	424.360525	7.084250
6.552994	425.205674	7.089254
6.058656	423.410587	7.094259
6.062064	423.972179	7.099264
6.525653	425.025114	7.104269
6.208910	425.381208	7.109274
6.294804	427.796753	7.114278
6.319488	429.348619	7.119283
6.441826	424.786161	7.124288
6.356340	429.690896	7.129293
6.275201	435.355061	7.134298
6.199101	419.329706	7.139302
6.066174	404.743494	7.144307
5.968120	399.299126	7.149312
6.083945	395.978814	7.154317
5.595009	419.225845	7.159322
5.684355	421.203515	7.164326
5.697391	426.665400	7.169331
6.140129	427.042944	7.174336
6.293821	424.174181	7.179341
6.083031	432.677610	7.184346
6.234264	423.950866	7.189350
6.386290	427.758931	7.194355
5.960318	422.056272	7.199360
6.234014	410.837000	7.204365
6.109785	416.618014	7.209370
6.295551	419.143908	7.214374
6.103817	427.847240	7.219379
5.845380	422.926123	7.224384
6.252370	426.031279	7.229389
6.070891	433.574539	7.234394
5.992024	421.101143	7.239398
6.215658	434.299543	7.244403
5.819541	428.087936	7.249408
5.900998	424.127025	7.254413
5.648727	430.309913	7.259418
5.811101	428.341745	7.264422
5.855064	429.435948	7.269427
5.904071	446.847445	7.274432
6.490164	440.556265	7.279437
6.290226	454.980833	7.284442
6.402021	439.557406	7.289446
6.306452	433.222223	7.294451
5.859931	432.455836	7.299456
5.882425	427.103388	7.304461
6.172269	434.227205	7.309466
6.238644	436.824970	7.314470
6.222864	424.289817	7.319475
6.008062	428.011214	7.324480
5.961072	427.301412	7.329485
6.021364	439.753495	7.334490
6.368725	442.157714	7.339494
6.385627	433.774673	7.344499
5.767210	429.252192	7.349504
6.227575	428.161184	7.354509
5.979029	430.935025	7.359514
6.452781	445.022467	7.364518
6.164224	426.312762	7.369523
5.672223	430.882440	7.374528
6.341690	441.070820	7.379533
6.388983	447.661342	7.384538
6.138599	428.620888	7.389542
6.176409	418.909462	7.394547
6.072491	428.418984	7.399552
6.120901	425.969435	7.404557
5.912154	422.114993	7.409562
5.870513	429.273966	7.414566
5.956598	444.497743	7.419571
6.139661	449.840902	7.424576
6.401752	447.900030	7.429581
6.389056	452.096902	7.434586
6.254891	444.178344	7.439590
6.090509	430.289975	7.444595
6.170047	429.236770	7.449600
6.226899	429.650981	7.454605
5.896079	426.736350	7.459610
6.254417	422.730380	7.464614
6.333172	427.015901	7.469619
5.763784	420.090010	7.474624
6.609707	418.182509	7.479629
6.299170	423.191603	7.484634
6.195851	435.946261	7.489638
6.254362	422.666089	7.494643
5.972017	430.965280	7.499648
6.153879	427.265793	7.504653
5.651451	433.576540	7.509658
5.715222	428.937344	7.514662
6.414188	439.475652	7.519667
6.373668	441.103439	7.524672
6.118292	430.584697	7.529677
6.206971	437.086467	7.534682
6.018939	437.626677	7.539686
6.278165	424.690183	7.544691
5.939979	433.575640	7.549696
6.158082	422.248742	7.554701
6.125332	433.188433	7.559706
6.158780	425.614310	7.564710
6.307040	420.432851	7.569715
5.849153	421.553520	7.574720
6.610649	422.971338	7.579725
6.044921	421.678458	7.584730
6.233481	419.012903	7.589734
6.018465	423.697346	7.594739
6.258146	423.763172	7.599744
6.297708	415.550441	7.604749
6.039834	421.915607	7.609754
6.018115	414.543819	7.614758
6.291927	426.152236	7.619763
6.057762	419.597283	7.624768
6.343784	413.344358	7.629773
6.136691	423.594403	7.634778
6.048729	420.750067	7.639782
6.287652	417.810950	7.644787
6.595648	424.588784	7.649792
6.116141	423.003971	7.654797
6.331648	425.195189	7.659802
6.265339	424.363473	7.664806
6.205285	424.918998	7.669811
6.027958	421.698138	7.674816
6.172653	416.807161	7.679821
6.125075	426.892065	7.684826
6.182984	425.384419	7.689830
6.175140	424.784762	7.694835
6.253260	427.477868	7.699840
6.236839	427.734107	7.704845
6.034471	429.867831	7.709850
6.065737	430.390868	7.714854
6.172326	422.535860	7.719859
6.313573	431.814354	7.724864
6.362260	421.596925	7.729869
6.106883	429.929145	7.734874
6.046746	425.817431	7.739878
6.035477	423.698243	7.744883
5.917390	442.216450	7.749888
6.046834	426.887402	7.754893
6.054982	433.685883	7.759898
6.035379	424.386334	7.764902
6.083682	429.766997	7.769907
5.871348	433.263811	7.774912
6.306038	430.180383	7.779917
6.002402	432.402510	7.784922
6.255232	426.602245	7.789926
6.195654	426.754726	7.794931
6.067452	426.096064	7.799936
6.142563	424.403032	7.804941
6.022587	428.212329	7.809946
5.817232	424.329895	7.814950
6.225024	425.579936	7.819955
6.364020	425.171062	7.824960
6.515000	423.535916	7.829965
5.915786	434.004430	7.834970
6.256681	427.993822	7.839974
5.884971	429.528840	7.844979
5.801069	428.199390	7.849984
6.080315	421.350833	7.854989
6.083798	434.897878	7.859994
5.810998	425.541981	7.864998
5.998728	421.896581	7.870003
5.890470	431.272830	7.875008
5.881197	420.378656	7.880013
5.952236	431.244326	7.885018
6.315493	437.996043	7.890022
6.501361	428.546037	7.895027
6.367437	434.958962	7.900032
6.137841	431.703144	7.905037
6.261710	422.265382	7.910042
6.082668	428.671567	7.915046
6.231279	421.041277	7.920051
5.826078	426.996302	7.925056
6.155347	430.613594	7.930061
6.288544	428.448184	7.935066
5.974238	429.265252	7.940070
6.329276	430.578889	7.945075
6.160510	430.998887	7.950080
6.202169	428.235109	7.955085
6.233391	435.214873	7.960090
6.129984	431.810480	7.965094
6.517856	429.700975	7.970099
6.266207	429.827244	7.975104
6.349811	422.614037	7.980109
6.119154	435.022731	7.985114
6.103345	428.601721	7.990118
6.361743	425.017877	7.995136
6.163845	430.722390	8.000154
6.348286	431.032510	8.005171
6.303527	429.043364	8.010189
6.725970	418.633607	8.015206
6.373363	405.728983	8.020224
5.715319	400.560554	8.025242
5.884709	408.060193	8.030259
6.417370	424.078340	8.035277
6.477223	418.138322	8.040294
6.365804	398.926934	8.045312
6.107054	403.144193	8.050330
6.121983	391.660294	8.055347
6.026221	401.304653	8.060365
5.932042	394.848855	8.065382
6.083864	411.440642	8.070400
5.923297	426.864193	8.075418
6.428959	432.167185	8.080435
6.551711	429.072431	8.085453
6.331994	427.365781	8.090470
6.057644	411.245096	8.095488
6.336628	420.945907	8.100506
6.181284	411.246352	8.105523
6.072673	420.284041	8.110541
6.215370	423.616192	8.115558
6.515231	427.815162	8.120576
6.107078	432.471309	8.125594
6.325503	426.221193	8.130611
6.295612	425.605069	8.135629
6.137375	433.035558	8.140646
6.283622	425.889393	8.145664
6.152264	440.394216	8.150682
6.206354	433.944949	8.155699
6.337890	432.199029	8.160717
6.032869	427.178416	8.165734
6.112230	428.643249	8.170752
6.154126	438.756925	8.175770
6.200063	440.836696	8.180787
6.001169	429.248621	8.185805
6.248549	436.804449	8.190822
6.448707	428.276825	8.195840
6.322922	433.381451	8.200858
6.406309	430.978202	8.205875
6.304726	434.784434	8.210893
6.285795	435.407934	8.215910
6.524854	426.255216	8.220928
6.037311	435.205673	8.225946
6.295220	431.588380	8.230963
6.694462	424.784347	8.235981
6.462187	429.996167	8.240998
6.341451	423.627031	8.246016
6.324420	435.073587	8.251034
6.442099	426.917862	8.256051
6.498823	425.080205	8.261069
6.382394	428.436764	8.266086
6.574650	426.146973	8.271104
6.491377	428.979381	8.276122
6.376940	430.910721	8.281139
6.476047	423.490300	8.286157
6.326424	427.429672	8.291174
6.705799	427.465208	8.296192
6.451350	430.264746	8.301210
6.291264	430.618336	8.306227
6.396538	430.106197	8.311245
5.866454	434.682347	8.316262
6.169608	433.254832	8.321280
6.254575	440.566711	8.326298
6.281991	449.676177	8.331315
6.787020	447.017882	8.336333
6.651403	454.590884	8.341350
6.805416	438.865933	8.346368
6.451649	437.276354	8.351386
6.322721	433.759532	8.356403
6.383326	435.283373	8.361421
6.674113	446.539999	8.366438
6.697838	434.156453	8.371456
6.365763	435.709495	8.376474
6.427744	429.413242	8.381491
6.392484	424.503262	8.386509
6.372555	450.539139	8.391526
6.450825	450.152918	8.396544
6.819246	455.313303	8.401562
6.656980	449.728534	8.406579
6.350506	447.864016	8.411597
6.457724	454.922631	8.416614
6.895315	459.801899	8.421632
6.949793	456.905636	8.426650
6.412666	449.208500	8.431667
6.512089	443.221765	8.436685
6.487060	438.106953	8.441702
6.600487	444.679729	8.446720
6.480658	453.824208	8.451738
6.568421	454.351504	8.456755
6.955711	456.734567	8.461773
6.597273	452.343610	8.466790
6.686846	438.975608	8.471808
6.550983	441.504546	8.476826
6.472931	446.622532	8.481843
6.308522	455.120507	8.486861
6.456258	461.013448	8.491878
6.641439	458.927958	8.496896
6.589652	458.346952	8.501914
6.536847	458.670770	8.506931
6.696745	456.972115	8.511949
6.663322	461.070390	8.516966
6.594693	457.009563	8.521984
6.246809	457.979837	8.527002
6.387920	457.021442	8.532019
6.551210	459.106190	8.537037
6.480049	462.068675	8.542054
6.668486	456.641955	8.547072
6.639075	458.166138	8.552090
6.675419	459.803046	8.557107
7.164710	457.729792	8.562125
6.612058	458.577883	8.567143
6.843033	453.706479	8.572160
6.840137	455.209147	8.577178
6.228722	466.383510	8.582195
6.813152	458.138274	8.587213
6.607186	457.902066	8.592231
7.016196	464.977634	8.597248
7.162216	465.506306	8.602266
6.815338	463.993726	8.607283
7.054957	449.532839	8.612301
6.574774	459.120232	8.617319
6.848708	456.080354	8.622336
6.879041	453.440629	8.627354
6.730007	463.179275	8.632371
7.014642	453.484980	8.637389
6.650566	460.822805	8.642407
6.791655	460.855874	8.647424
6.889739	459.128088	8.652442
6.722104	457.855099	8.657459
7.153004	457.576615	8.662477
6.926474	461.092937	8.667495
6.931505	455.363148	8.672512
7.370471	456.248201	8.677530
6.993542	459.478821	8.682547
7.245611	452.922162	8.687565
7.209251	456.690042	8.692583
7.377078	457.955007	8.697600
6.944466	453.142310	8.702618
6.739377	437.555756	8.707635
6.626620	433.119004	8.712653
6.565436	452.191981	8.717671
6.494714	463.412034	8.722688
7.000160	453.112713	8.727706
6.786847	450.942830	8.732723
7.014251	448.933611	8.737741
6.833498	452.877751	8.742759
6.891618	456.254620	8.747776
6.949311	455.179734	8.752794
6.814318	453.204542	8.757811
7.257743	449.881106	8.762829
7.035171	455.366306	8.767847
6.996147	457.435151	8.772864
6.944709	469.709809	8.777882
6.863481	464.343880	8.782899
6.715924	456.229502	8.787917
6.668145	458.180513	8.792935
7.109700	461.514164	8.797952
7.088004	458.359669	8.802970
6.874560	465.630627	8.807987
7.118392	453.388163	8.813005
7.150769	461.673451	8.818023
7.098030	457.118101	8.823040
7.154084	457.251859	8.828058
7.117759	457.461342	8.833075
7.042631	455.918330	8.838093
7.004467	460.826580	8.843111
6.850503	460.189664	8.848128
7.124682	451.679886	8.853146
6.726759	462.183509	8.858163
7.084007	458.462365	8.863181
6.779773	461.169963	8.868199
7.032033	458.464750	8.873216
7.156222	457.973689	8.878234
6.597793	455.782613	8.883251
6.767537	464.340212	8.888269
6.951182	484.339149	8.893287
7.207681	485.727809	8.898304
7.420657	483.274748	8.903322
7.052795	491.886349	8.908339
7.582601	489.930388	8.913357
7.568657	487.459002	8.918375
6.894059	463.709442	8.923392
7.087628	469.947920	8.928410
7.428678	473.880062	8.933427
7.463813	463.965087	8.938445
6.915547	462.627578	8.943463
7.201631	463.802296	8.948480
7.142700	457.156988	8.953498
7.059001	468.280972	8.958515
7.160583	469.220122	8.963533
7.112155	480.439644	8.968551
7.604613	482.809233	8.973568
7.397594	466.322840	8.978586
7.107214	461.741097	8.983603
7.117093	458.226282	8.988621
7.248737	460.142071	8.993639
7.031139	459.684184	8.998656
7.070485	470.156346	9.003674
7.221899	486.729189	9.008691
7.287598	487.545551	9.013709
7.447075	486.804372	9.018727
7.322858	487.621083	9.023744
7.325489	474.374920	9.028762
6.956599	481.995224	9.033779
6.881890	488.102950	9.038797
7.310716	487.462631	9.043815
7.055077	489.832881	9.048832
7.119749	492.841772	9.053850
7.577368	500.836798	9.058867
7.341827	489.644875	9.063885
7.347295	498.867051	9.068903
7.213227	489.754234	9.073920
7.244427	494.404176	9.078938
7.090894	494.707276	9.083955
7.129322	491.913263	9.088973
7.390127	493.788182	9.093991
7.148175	489.122630	9.099008
7.400559	492.286053	9.104026
7.361049	494.453597	9.109043
7.087793	490.694146	9.114061
7.247560	487.281856	9.119079
6.953723	495.585948	9.124096
7.618710	501.995176	9.129114
7.376401	498.187885	9.134131
7.306264	493.544072	9.139149
7.528467	504.515073	9.144167
7.299642	508.638631	9.149184
7.452719	518.550497	9.154202
7.534161	519.732732	9.159219
7.733089	514.983929	9.164237
7.615214	503.640237	9.169255
7.454529	498.209311	9.174272
7.564047	491.267413	9.179290
7.391751	492.912497	9.184307
7.671334	494.059950	9.189325
7.647146	495.319316	9.194343
7.469050	497.785183	9.199360
7.447560	486.033446	9.204378
7.440072	486.207645	9.209395
7.601012	486.117751	9.214413
7.673904	483.683950	9.219431
7.528845	498.552683	9.224448
7.568214	497.517833	9.229466
7.394570	496.426334	9.234483
7.581497	478.949958	9.239501
7.629650	486.275435	9.244519
7.465727	490.848837	9.249536
7.656980	478.288509	9.254554
7.808055	491.234715	9.259571
7.839159	482.009912	9.264589
7.942786	484.313190	9.269607
7.665366	500.243922	9.274624
7.623993	487.389061	9.279642
7.871109	493.755680	9.284659
7.667607	486.278259	9.289677
7.998669	491.007670	9.294695
7.854472	492.778801	9.299712
7.702873	483.139599	9.304730
7.143366	488.954206	9.309747
7.965493	487.028378	9.314765
7.761992	484.967683	9.319783
7.476408	494.468153	9.324800
7.457522	495.978787	9.329818
7.498485	489.023244	9.334835
7.557534	491.630339	9.339853
7.924132	486.811067	9.344871
7.783849	503.045447	9.349888
7.877100	486.973056	9.354906
7.466362	494.904014	9.359923
7.351680	499.435803	9.364941
7.611454	493.633110	9.369959
7.537595	502.912318	9.374976
7.490255	491.451845	9.379994
7.581903	495.652637	9.385011
7.503932	492.361795	9.390029
7.401148	496.074744	9.395047
7.319410	492.755197	9.400064
7.390714	501.331480	9.405082
7.714533	523.724402	9.410099
7.947583	525.272449	9.415117
8.043057	522.720344	9.420135
7.565266	527.405963	9.425152
7.822149	513.556287	9.430170
7.811352	524.160992	9.435187
7.719528	526.563959	9.440205
7.845126	523.619492	9.445223
7.916626	534.765655	9.450240
8.120277	520.949983	9.455258
8.131935	510.596377	9.460275
7.673566	504.974012	9.465293
7.498641	498.174875	9.470311
7.833412	519.270600	9.475328
7.958233	527.381768	9.480346
7.795680	528.286516	9.485363
7.746697	526.324236	9.490381
8.055132	522.634190	9.495399
7.802913	522.370209	9.500416
8.047879	521.478268	9.505434
7.893364	524.543144	9.510451
7.910265	522.817378	9.515469
8.223044	518.601257	9.520487
7.604536	514.066156	9.525504
7.916961	520.902645	9.530522
7.885963	521.962761	9.535539
7.549274	524.450170	9.540557
7.546142	519.617315	9.545575
7.406253	524.103091	9.550592
7.726414	522.404464	9.555610
7.963362	520.276342	9.560627
7.875712	519.540457	9.565645
8.117708	520.600049	9.570663
7.858404	522.465828	9.575680
7.878971	525.063948	9.580698
7.903479	522.965295	9.585715
7.702551	522.424337	9.590733
8.126356	528.118450	9.595751
7.948559	546.064871	9.600768
8.077395	541.082015	9.605786
8.200287	540.007743	9.610803
7.641847	533.686044	9.615821
7.884688	541.112566	9.620839
8.232564	556.375285	9.625856
8.234193	552.932479	9.630874
8.487476	556.328821	9.635891
8.214905	540.693499	9.640909
8.258862	524.422553	9.645927
8.109653	531.238252	9.650944
7.963120	533.681380	9.655962
8.013503	527.431493	9.660979
7.857321	524.735837	9.665997
8.007326	533.885283	9.671015
8.012719	549.596609	9.676032
8.131566	547.320728	9.681050
8.319805	561.317458	9.686067
8.276498	561.907994	9.691085
8.318835	542.674116	9.696103
7.944175	538.958805	9.701120
8.157780	540.333314	9.706138
8.297315	554.512302	9.711155
7.665019	550.792606	9.716173
8.189081	555.949101	9.721191
8.333938	560.152320	9.726208
8.402073	552.498793	9.731226
8.235037	553.820594	9.736243
8.150683	550.322741	9.741261
8.462837	554.065017	9.746279
8.324460	546.380340	9.751296
8.094623	538.333870	9.756314
8.479469	549.842301	9.761331
8.269113	547.331780	9.766349
8.205407	528.481399	9.771367
8.206450	534.849218	9.776384
7.783881	550.507208	9.781402
8.517740	551.354654	9.786419
8.197458	557.023578	9.791437
8.268008	558.456224	9.796455
8.399960	570.103390	9.801472
8.434863	570.737665	9.806490
8.567906	555.876836	9.811507
8.182884	551.926836	9.816525
8.357357	551.409533	9.821543
8.407871	561.851367	9.826560
8.117148	557.148007	9.831578
8.327149	553.148685	9.836595
8.120582	561.787352	9.841613
8.111713	559.911332	9.846631
8.201285	564.708115	9.851648
8.361646	562.310602	9.856666
8.566819	562.121853	9.861683
8.525877	563.909750	9.866701
8.538060	560.090614	9.871719
8.237983	566.055387	9.876736
8.336873	564.383358	9.881754
8.701840	559.805262	9.886771
8.198678	560.865816	9.891789
8.489338	551.604881	9.896807
8.478647	553.445833	9.901824
8.093999	565.182084	9.906842
8.397004	565.577882	9.911859
8.659385	569.531146	9.916877
8.641352	561.144100	9.921895
8.609736	561.228995	9.926912
8.408114	564.924865	9.931930
8.479858	555.945042	9.936947
8.409871	565.093537	9.941965
8.433718	560.172940	9.946983
8.291912	567.880674	9.952000
8.498495	564.281101	9.957018
8.587931	563.866849	9.962035
8.072495	561.855633	9.967053
8.386370	559.803540	9.972071
8.485380	552.212415	9.977088
8.448583	557.280301	9.982106
8.787562	560.211698	9.987123
8.831993	561.069182	9.992141
8.518152	561.119517	9.997159
8.414972	567.981149	10.002176
8.277732	567.815443	10.007194
8.742145	562.971486	10.012211
8.451705	576.321560	10.017229
8.543006	585.829554	10.022247
8.767274	578.377703	10.027264
8.654130	586.634403	10.032282
9.151480	578.093112	10.037299
8.832393	575.895060	10.042317
8.541302	562.190408	10.047335
8.785892	561.868566	10.052352
8.576438	561.178241	10.057370
8.720647	562.857727	10.062387
8.792125	568.941277	10.067405
8.767518	563.504328	10.072423
8.726218	560.417621	10.077440
8.595042	567.634062	10.082458
8.704488	563.668907	10.087475
8.672290	565.592748	10.092493
8.527294	554.232842	10.097511
8.595998	564.519117	10.102528
8.496616	580.603311	10.107546
8.616999	582.692820	10.112563
8.899840	581.457619	10.117581
8.881626	588.004817	10.122599
9.265907	573.603712	10.127616
9.004377	568.961258	10.132634
8.812604	561.237780	10.137651
8.651498	564.727742	10.142669
8.423452	564.165093	10.147687
8.810726	571.039797	10.152704
8.709424	578.879599	10.157722
9.307096	578.944732	10.162739
9.128411	578.794943	10.167757
8.803312	573.596910	10.172775
8.696007	566.314137	10.177792
8.390192	566.313737	10.182810
8.835756	574.413941	10.187827
8.310888	589.242511	10.192845
8.518763	582.729333	10.197863
8.864756	586.824849	10.202880
8.754271	581.492069	10.207898
8.948919	591.833289	10.212915
8.918460	588.253278	10.217933
8.731015	585.443702	10.222951
9.072195	577.394579	10.227968
8.816187	585.100171	10.232986
8.643978	585.973846	10.238003
8.398852	588.346307	10.243021
8.687431	601.996558	10.248039
8.678198	603.539854	10.253056
8.701889	619.887352	10.258074
8.991895	613.850489	10.263091
8.975692	612.888806	10.268109
9.322264	611.328504	10.273127
9.584256	607.267413	10.278144
9.328547	623.440920	10.283162
9.547984	604.829171	10.288179
9.079725	599.209196	10.293197
9.192322	593.657003	10.298215
8.798836	576.081564	10.303232
8.643771	591.450237	10.308250
9.240807	604.268756	10.313267
9.144789	618.760610	10.318285
9.186198	614.317567	10.323303
9.595029	595.224891	10.328320
9.169627	591.589028	10.333338
9.134809	586.646051	10.338355
9.022798	584.261947	10.343373
9.186447	586.444088	10.348391
9.184375	580.004453	10.353408
8.823067	584.736544	10.358426
9.080646	583.856290	10.363443
8.924160	591.498362	10.368461
8.795198	601.095591	10.373479
9.275962	607.488719	10.378496
9.161762	618.618846	10.383514
9.218383	614.709273	10.388531
9.327515	614.408286	10.393549
9.266306	607.387527	10.398567
9.340989	608.934053	10.403584
9.190776	611.851393	10.408602
9.451042	611.042538	10.413619
9.523481	617.900700	10.418637
9.435975	609.298179	10.423655
9.307731	585.302261	10.428672
9.228083	582.321302	10.433690
9.166876	576.572912	10.438707
9.332302	580.205052	10.443725
9.166185	584.275533	10.448743
9.476532	578.330585	10.453760
9.322163	586.907673	10.458778
9.282800	583.116948	10.463795
9.205596	580.892620	10.468813
9.207368	594.442730	10.473831
9.661293	599.438228	10.478848
9.281527	600.268523	10.483866
9.451157	589.244458	10.488883
9.201145	583.721411	10.493901
9.314771	598.918638	10.498919
9.469623	600.089510	10.503936
9.187405	603.211372	10.508954
9.285744	610.341209	10.513971
9.275190	608.786700	10.518989
9.185389	621.826246	10.524007
9.721993	618.501517	10.529024
9.188219	613.040211	10.534042
9.556729	608.833733	10.539059
9.714813	615.941672	10.544077
9.587568	614.970032	10.549095
9.767422	620.003637	10.554112
9.515796	612.145567	10.559130
9.309888	604.168126	10.564147
9.707790	602.591451	10.569165
9.585081	603.350442	10.574183
9.248914	603.767639	10.579200
9.322443	601.006571	10.584218
9.366749	614.161885	10.589235
9.592753	613.641165	10.594253
9.249411	615.688184	10.599271
9.832756	599.860089	10.604288
9.534689	609.468791	10.609306
9.360368	611.947436	10.614323
9.576360	610.664842	10.619341
9.527312	615.811542	10.624359
9.301956	618.180143	10.629376
9.387791	611.432454	10.634394
9.660146	605.373126	10.639411
9.891954	607.213100	10.644429
9.656394	617.076399	10.649447
9.584369	602.863813	10.654464
9.714908	607.730198	10.659482
9.539717	620.769710	10.664499
9.421613	616.782384	10.669517
9.558099	607.540056	10.674535
9.926099	608.568553	10.679552
9.650893	609.669311	10.684570
9.649979	613.585680	10.689587
9.675287	604.857990	10.694605
9.679049	610.612242	10.699623
9.726989	607.745378	10.704640
9.764867	604.509339	10.709658
9.603534	601.330499	10.714675
9.530157	603.507210	10.719693
9.664726	618.838578	10.724711
9.839707	607.673859	10.729728
9.610199	610.280139	10.734746
9.634801	616.005352	10.739763
9.770957	617.143103	10.744781
9.879140	631.983217	10.749799
9.797023	621.588376	10.754816
9.782293	620.625662	10.759834
9.787212	623.033292	10.764851
9.884950	621.513602	10.769869
9.803733	635.885903	10.774887
9.990764	636.100723	10.779904
9.528712	634.457404	10.784922
9.709726	636.140449	10.789939
9.846100	641.090125	10.794957
10.137249	648.938004	10.799975
10.060034	640.038504	10.804992
10.020147	647.238881	10.810010
9.885813	641.711224	10.815027
10.198137	635.322648	10.820045
9.652229	628.486860	10.825063
9.803977	636.590871	10.830080
9.544047	637.808778	10.835098
9.513862	642.417556	10.840115
9.745662	642.675746	10.845133
9.548783	643.644646	10.850151
9.728736	637.055563	10.855168
9.940486	643.794217	10.860186
9.722141	642.549884	10.865203
9.872055	646.742250	10.870221
9.966529	649.211231	10.875239
10.036672	656.999653	10.880256
10.224453	666.912954	10.885274
10.010040	667.996562	10.890291
10.364931	649.693018	10.895309
10.061631	649.064682	10.900327
10.195677	636.827655	10.905344
10.159076	640.960360	10.910362
10.176863	639.485206	10.915379
10.192408	639.176489	10.920397
10.039698	645.240110	10.925415
10.521200	637.136620	10.930432
10.502303	638.344533	10.935450
10.196913	642.156810	10.940467
10.433566	640.480857	10.945485
10.033375	634.015005	10.950503
10.081712	637.240395	10.955520
10.114893	641.121009	10.960538
9.663247	642.193509	10.965555
10.268300	635.540332	10.970573
10.192726	636.264355	10.975591
10.406501	633.241884	10.980608
10.364812	631.062452	10.985626
10.247326	635.380192	10.990643
10.500769	628.659659	10.995661
10.673561	635.472473	11.000679
10.487495	639.493322	11.005696
10.542775	636.341201	11.010714
10.175224	633.637419	11.015731
10.247991	630.438311	11.020749
10.374208	635.800665	11.025767
10.304091	627.300365	11.030784
10.309776	635.238024	11.035802
10.419050	639.184378	11.040819
10.569644	633.742211	11.045837
10.365677	633.021054	11.050855
10.527105	636.337552	11.055872
10.376456	625.893628	11.060890
10.108934	631.921141	11.065907
10.675394	635.626444	11.070925
10.526305	638.751070	11.075943
10.456023	633.049828	11.080960
10.515385	631.041839	11.085978
10.427354	633.749687	11.090995
10.404170	618.509379	11.096013
10.442440	625.515713	11.101031
10.208935	618.879953	11.106048
10.546490	625.567651	11.111066
10.233325	639.248293	11.116083
10.367282	634.476160	11.121101
10.498373	632.452750	11.126119
10.176101	634.120716	11.131136
10.657992	633.395429	11.136154
10.404176	637.457809	11.141171
10.535503	643.362198	11.146189
10.728091	631.972119	11.151207
10.488290	639.972870	11.156224
10.561648	635.242266	11.161242
10.679371	637.220812	11.166259
10.735583	628.514172	11.171277
10.386713	638.933221	11.176295
10.066956	637.745442	11.181312
10.501979	632.826612	11.186330
10.071174	631.318661	11.191347
10.385298	633.356411	11.196365
10.200660	640.313449	11.201383
10.354048	644.339896	11.206400
10.541745	650.556979	11.211418
10.339828	667.122977	11.216435
10.637645	662.320946	11.221453
10.831218	669.833046	11.226471
10.578233	671.680081	11.231488
10.334618	666.978335	11.236506
10.202423	667.769606	11.241523
10.476171	658.644667	11.246541
10.739895	659.928609	11.251559
10.429065	664.335850	11.256576
10.511699	666.263521	11.261594
10.567006	662.432298	11.266611
10.573406	664.507230	11.271629
10.756527	688.175185	11.276647
10.799427	693.900547	11.281664
10.972548	690.655677	11.286682
10.739111	691.244830	11.291699
11.151811	687.008378	11.296717
10.948341	681.708283	11.301735
10.432165	676.346986	11.306752
10.921471	677.451852	11.311770
11.111628	686.316805	11.316787
10.775212	667.347841	11.321805
11.184491	669.888310	11.326823
10.763447	670.160125	11.331840
10.995092	662.688903	11.336858
10.464187	673.589272	11.341875
10.742304	674.416136	11.346893
11.073417	683.536863	11.351911
10.942888	695.825583	11.356928
10.854151	688.130647	11.361946
11.269490	693.599466	11.366963
10.990946	683.821131	11.371981
11.013524	675.724327	11.376999
10.950430	674.109422	11.382016
11.257677	662.987324	11.387034
10.785895	662.379407	11.392051
10.930938	658.654972	11.397069
11.349202	665.746816	11.402087
11.007181	675.346303	11.407104
11.026751	667.346846	11.412122
10.755882	668.885051	11.417139
11.031467	670.362294	11.422157
11.025742	671.688887	11.427175
10.824277	682.790206	11.432192
10.964969	689.801655	11.437210
10.906004	683.843024	11.442227
11.197154	696.790614	11.447245
11.310411	692.791530	11.452263
11.232302	697.355507	11.457280
11.170928	694.408900	11.462298
11.188439	699.406229	11.467315
10.990539	702.875150	11.472333
11.308888	705.522803	11.477351
11.034251	701.934778	11.482368
11.364163	694.392941	11.487386
10.799423	699.196153	11.492403
11.114136	693.970080	11.497421
11.218604	695.001280	11.502439
10.950419	691.515332	11.507456
10.981740	691.842152	11.512474
11.095908	697.296675	11.517491
11.259978	702.348471	11.522509
11.140154	697.140812	11.527527
11.367952	703.784322	11.532544
11.116472	693.470822	11.537562
11.246043	696.620965	11.542579
11.509044	696.134271	11.547597
11.498677	689.834933	11.552615
11.420970	696.976245	11.557632
11.853358	694.141564	11.562650
11.379528	696.634191	11.567667
11.582595	694.861831	11.572685
11.601678	693.335279	11.577703
11.390451	700.742782	11.582720
11.520638	689.575187	11.587738
11.671077	696.796429	11.592755
11.350664	695.963064	11.597773
11.821541	690.259979	11.602791
11.604812	677.960934	11.607808
11.453152	673.827387	11.612826
11.084855	665.878379	11.617843
11.534910	664.954832	11.622861
11.798009	670.375628	11.627879
11.582636	666.537655	11.632896
11.194485	659.990670	11.637914
11.262434	669.827759	11.642931
11.664802	679.654356	11.647949
11.849699	673.226633	11.652967
10.891170	674.624001	11.657984
11.108817	679.759038	11.663002
11.933210	692.271889	11.668019
11.509503	694.027126	11.673037
11.691398	677.489098	11.678055
11.328319	691.269777	11.683072
11.456663	691.497072	11.688090
11.720943	692.578575	11.693107
11.365698	700.863025	11.698125
11.360627	685.584614	11.703143
11.528512	700.151734	11.708160
11.840874	683.829876	11.713178
11.604582	694.161034	11.718195
11.593099	695.608261	11.723213
11.809065	684.488271	11.728231
11.581791	696.771361	11.733248
11.746830	687.289626	11.738266
11.836703	695.138969	11.743283
11.703187	698.567703	11.748301
11.580906	687.522619	11.753319
11.325614	701.787397	11.758336
11.461371	695.882338	11.763354
11.601295	689.717552	11.768371
11.459854	695.275027	11.773389
11.581961	700.810514	11.778407
11.620739	719.793256	11.783424
11.862661	720.335188	11.788442
11.752549	726.542959	11.793459
12.037439	728.902080	11.798477
12.174054	717.555457	11.803495
11.681672	724.255636	11.808512
11.690694	728.413485	11.813530
11.897228	723.300192	11.818547
11.957630	723.222615	11.823565
12.146697	718.124420	11.828583
11.672580	723.919266	11.833600
12.106803	721.172460	11.838618
12.046825	732.044492	11.843635
11.878046	724.210832	11.848653
11.924139	711.078522	11.853671
11.793157	706.843123	11.858688
11.777380	721.487917	11.863706
11.859464	725.843103	11.868723
11.619408	717.340187	11.873741
11.870041	721.572586	11.878759
11.765779	723.696163	11.883776
11.581235	725.092527	11.888794
11.763098	725.492446	11.893811
11.756935	724.933400	11.898829
11.916731	718.933806	11.903847
12.010052	728.888771	11.908864
11.957632	752.527329	11.913882
12.040041	748.741988	11.918899
12.077528	755.659539	11.923917
12.107593	752.152928	11.928935
12.101754	755.563681	11.933952
12.118093	751.184196	11.938970
12.347979	747.975188	11.943987
12.345843	750.236967	11.949005
12.256401	739.785586	11.954023
12.123477	736.580756	11.959040
12.393035	739.226259	11.964058
12.374072	732.885809	11.969075
12.055682	725.480837	11.974093
12.237845	718.734669	11.979111
11.984215	727.927843	11.984128
12.349502	740.403772	11.989146
12.696460	738.269804	11.994163
12.362286	729.921435	11.999181
12.275148	719.166161	12.004199
12.501028	714.058722	12.009216
12.062770	714.595183	12.014234
12.205790	717.763181	12.019251
11.953665	717.985372	12.024269
12.510861	733.184472	12.029287
12.166436	731.765745	12.034304
12.112827	749.557987	12.039322
12.388903	742.646266	12.044339
12.307248	753.857316	12.049357
12.501787	750.348272	12.054375
12.378718	746.551290	12.059392
12.413581	746.291732	12.064410
12.716462	751.347329	12.069427
12.414304	753.444628	12.074445
12.578457	746.262480	12.079463
12.716724	742.611190	12.084480
12.063468	744.812687	12.089498
12.272121	749.554772	12.094515
12.557627	751.618929	12.099533
12.594693	748.659160	12.104551
12.325417	744.273432	12.109568
12.271146	745.541932	12.114586
13.028403	745.382425	12.119603
12.631804	754.497325	12.124621
12.608659	751.306989	12.129639
12.362092	750.436196	12.134656
12.511469	758.630817	12.139674
13.242854	745.092497	12.144691
12.724586	744.163946	12.149709
12.574666	729.107892	12.154727
12.861377	716.281383	12.159744
12.619230	723.690474	12.164762
12.443469	710.502388	12.169779
12.467091	733.329160	12.174797
12.502424	740.960799	12.179815
12.849972	746.536133	12.184832
12.603761	741.620632	12.189850
12.782377	738.655535	12.194867
12.791879	747.822863	12.199885
12.852303	755.677508	12.204903
12.751207	749.818342	12.209920
12.687571	742.968386	12.214938
13.171973	740.997081	12.219955
12.830403	735.887149	12.224973
12.579876	730.182255	12.229991
12.473758	729.700387	12.235008
12.431481	749.124121	12.240026
12.902637	739.816454	12.245043
12.591546	743.975743	12.250061
12.286622	752.493605	12.255079
12.884827	750.175126	12.260096
12.770362	747.682551	12.265114
12.992695	748.906429	12.270131
12.907177	761.190504	12.275149
12.668300	752.491322	12.280167
12.744999	750.028898	12.285184
12.497378	745.974211	12.290202
12.725292	747.027096	12.295219
12.687905	770.833655	12.300237
12.930594	774.038307	12.305255
13.193429	770.301032	12.310272
12.927413	786.789193	12.315290
13.247505	776.285720	12.320307
13.234877	786.797213	12.325325
13.199779	779.090593	12.330343
13.259935	758.035094	12.335360
12.919933	760.745714	12.340378
13.290630	751.325549	12.345395
13.250058	751.593807	12.350413
12.659687	753.477036	12.355431
13.067224	749.104028	12.360448
13.169945	780.189742	12.365466
13.378751	764.943943	12.370483
13.196437	754.353216	12.375501
13.239181	757.448462	12.380519
13.664196	738.068301	12.385536
13.449241	748.571148	12.390554
13.141778	738.945982	12.395571
12.762893	737.793969	12.400589
12.831996	737.916514	12.405607
13.233822	746.976753	12.410624
13.216670	760.199059	12.415642
13.413608	755.287333	12.420659
13.050648	756.136505	12.425677
13.088426	760.062841	12.430695
13.432754	765.101344	12.435712
13.249516	778.536983	12.440730
13.111323	780.127241	12.445747
13.696011	783.315811	12.450765
13.068049	770.451360	12.455783
13.413977	774.021572	12.460800
13.382281	781.237583	12.465818
13.448436	781.685402	12.470835
13.773163	782.325036	12.475853
13.049739	760.181245	12.480871
12.981676	765.137650	12.485888
12.947980	773.470855	12.490906
12.957322	772.045509	12.495923
13.376303	786.024311	12.500941
13.100404	778.288672	12.505959
13.636695	776.093822	12.510976
13.547187	788.047888	12.515994
13.832626	781.931407	12.521011
13.806811	784.699053	12.526029
13.536551	781.801979	12.531047
13.497601	772.602382	12.536064
13.379639	781.143235	12.541082
13.553958	783.735229	12.546099
13.371032	778.850967	12.551117
13.362290	780.287512	12.556135
13.598068	773.889116	12.561152
13.444542	773.855230	12.566170
13.416261	779.083383	12.571187
13.508562	773.376426	12.576205
13.425920	778.751762	12.581223
13.753471	774.157753	12.586240
13.643630	790.150792	12.591258
13.633186	783.968351	12.596275
14.017993	780.895090	12.601293
13.809608	782.080459	12.606311
13.805854	781.695018	12.611328
13.601609	776.609180	12.616346
13.675685	776.526583	12.621363
13.737044	779.142399	12.626381
13.458328	777.268323	12.631399
14.227555	786.385850	12.636416
13.763908	786.186400	12.641434
13.650612	781.283521	12.646451
13.602289	785.011535	12.651469
13.649605	795.519013	12.656487
13.877070	793.432382	12.661504
14.012568	801.305719	12.666522
13.690867	802.098851	12.671539
13.920273	799.619400	12.676557
13.867801	803.578801	12.681575
14.014922	803.083736	12.686592
13.555176	805.260678	12.691610
13.764111	800.337110	12.696627
13.806447	805.644912	12.701645
13.944033	800.795360	12.706663
14.034222	797.970478	12.711680
13.920723	802.616326	12.716698
13.736286	797.153206	12.721715
14.129087	809.693922	12.726733
13.978409	797.375577	12.731751
14.389256	792.772495	12.736768
14.214200	807.511458	12.741786
13.945144	807.251441	12.746803
13.936904	808.883170	12.751821
13.839293	802.841134	12.756839
14.580711	797.371149	12.761856
14.020095	813.118794	12.766874
14.309106	804.140840	12.771891
14.463371	802.382455	12.776909
14.138577	809.454110	12.781927
14.195689	806.395740	12.786944
14.322959	809.528178	12.791962
13.890987	798.620906	12.796979
14.012572	797.621042	12.801997
13.734956	805.550585	12.807015
13.937670	796.668418	12.812032
14.030331	801.888362	12.817050
13.958282	803.960949	12.822067
14.048557	804.830343	12.827085
14.175652	829.579782	12.832103
14.552902	828.717098	12.837120
14.119693	832.748608	12.842138
14.232890	832.667012	12.847155
14.392674	834.018572	12.852173
14.148093	838.739284	12.857191
14.194652	833.187509	12.862208
14.379112	831.248933	12.867226
14.519647	829.262121	12.872243
14.304365	822.413620	12.877261
13.995536	830.151898	12.882279
14.341069	824.126625	12.887296
14.151846	832.287988	12.892314
14.369020	832.090754	12.897331
14.571664	832.238429	12.902349
14.546696	836.271233	12.907367
14.580162	826.974971	12.912384
14.411989	832.559754	12.917402
14.352857	838.005230	12.922419
14.644926	835.548466	12.927437
14.578507	833.233344	12.932455
14.471277	829.336479	12.937472
14.508201	832.965353	12.942490
14.348886	831.821460	12.947507
14.305040	832.907542	12.952525
14.602855	837.041219	12.957543
14.817635	844.933338	12.962560
14.756688	840.381202	12.967578
14.610406	833.831885	12.972595
14.762946	831.182489	12.977613
14.373031	840.362077	12.982631
14.646441	849.605050	12.987648
14.724344	853.605471	12.992666
14.621219	862.927337	12.997683
14.774187	858.355127	13.002701
14.859102	865.114881	13.007719
14.827483	868.707872	13.012736
14.857935	862.384776	13.017754
15.035912	861.347619	13.022771
15.264526	840.313323	13.027789
14.750048	839.052265	13.032807
14.935111	833.651562	13.037824
14.711544	829.477127	13.042842
14.849876	829.552778	13.047859
14.644558	829.595181	13.052877
14.600828	842.297182	13.057895
14.999560	847.765656	13.062912
15.123906	853.418932	13.067930
15.181233	866.605768	13.072947
15.065897	835.155334	13.077965
14.981887	832.404565	13.082983
14.879668	832.706260	13.088000
15.030471	824.085416	13.093018
14.889716	829.555821	13.098035
14.893037	839.164755	13.103053
14.894977	856.601482	13.108071
14.791336	859.695793	13.113088
15.176262	864.093385	13.118106
15.424127	867.428688	13.123123
15.416851	854.216123	13.128141
14.710645	850.268052	13.133159
14.893434	860.423630	13.138176
15.058301	858.218623	13.143194
14.942209	861.374442	13.148211
15.200627	856.049374	13.153229
14.883974	863.849591	13.158247
15.349554	858.855949	13.163264
15.130611	853.730002	13.168282
15.058594	867.542950	13.173299
15.548437	855.426354	13.178317
14.978307	859.134104	13.183335
15.186976	858.120996	13.188352
15.620413	854.667640	13.193370
15.402483	861.389751	13.198387
15.472700	857.914654	13.203405
15.207106	862.284540	13.208423
15.040178	856.103180	13.213440
15.278392	861.314396	13.218458
15.154772	869.184615	13.223475
15.335409	853.601679	13.228493
15.334890	850.864245	13.233511
15.484698	858.728942	13.238528
15.413063	858.579139	13.243546
15.170622	857.825367	13.248563
15.266763	850.124932	13.253581
15.214947	856.913229	13.258599
15.365040	857.335341	13.263616
15.529218	851.713297	13.268634
15.294150	860.501527	13.273651
15.494990	837.252260	13.278669
15.217699	861.575038	13.283687
15.548458	873.158412	13.288704
15.943266	884.575290	13.293722
15.607580	879.463942	13.298739
15.715189	859.488190	13.303757
15.747172	852.438896	13.308775
15.263237	855.567834	13.313792
15.714286	866.857282	13.318810
15.449752	884.279901	13.323827
15.664858	889.448105	13.328845
15.456681	887.766655	13.333863
15.562856	886.215427	13.338880
15.714664	884.357050	13.343898
15.769725	891.099319	13.348915
15.765646	883.876858	13.353933
15.689105	894.347041	13.358951
15.780989	886.724848	13.363968
15.778991	886.865861	13.368986
15.740335	889.649037	13.374003
15.996724	882.618867	13.379021
15.853875	891.260747	13.384039
15.683406	884.708327	13.389056
16.019378	889.349455	13.394074
15.892584	892.148014	13.399091
16.091047	876.645170	13.404109
15.896803	883.169676	13.409127
15.738384	892.777474	13.414144
15.703108	880.879302	13.419162
15.845164	892.203794	13.424179
15.780929	883.710647	13.429197
15.900409	885.583034	13.434215
15.512114	889.435870	13.439232
16.223952	883.225120	13.444250
15.984889	893.921024	13.449267
15.902558	889.583429	13.454285
15.764463	889.428095	13.459303
15.725758	888.779949	13.464320
16.032696	891.523614	13.469338
15.786494	904.113530	13.474355
15.802385	908.062032	13.479373
16.452893	916.063128	13.484391
16.375276	925.614656	13.489408
16.155955	916.277132	13.494426
15.687204	909.464266	13.499443
15.579301	917.101996	13.504461
15.858153	916.828015	13.509479
15.893223	916.892421	13.514496
16.272378	923.984169	13.519514
16.250330	922.954146	13.524531
16.343549	917.771369	13.529549
16.495718	916.641635	13.534567
16.547797	916.429221	13.539584
16.675722	916.023941	13.544602
15.966236	922.455838	13.549619
16.116945	916.847025	13.554637
16.741961	919.496688	13.559655
16.424596	924.228297	13.564672
16.562755	920.107713	13.569690
16.317890	914.099465	13.574707
16.567832	924.806538	13.579725
16.657368	919.466896	13.584743
16.333754	921.557141	13.589760
16.334608	916.102271	13.594778
16.360637	914.888312	13.599795
16.588891	906.192789	13.604813
16.538869	912.174946	13.609831
16.431687	921.268395	13.614848
16.303277	908.988005	13.619866
15.964543	914.550669	13.624883
16.143896	920.990100	13.629901
16.492144	916.274912	13.634919
16.258272	920.380124	13.639936
16.486507	934.657563	13.644954
16.355439	949.668892	13.649971
16.566692	947.611302	13.654989
16.812029	940.439636	13.660007
16.593230	951.981005	13.665024
16.733800	945.162497	13.670042
16.913441	945.113597	13.675059
16.797975	942.858546	13.680077
16.956962	942.235139	13.685095
16.879967	951.481081	13.690112
16.912445	941.451482	13.695130
17.079465	938.534722	13.700147
17.120613	918.237237	13.705165
17.049443	903.678973	13.710183
16.762914	895.469862	13.715200
17.188518	901.977164	13.720218
17.115078	903.924016	13.725235
17.400535	905.118559	13.730253
17.312056	904.995952	13.735271
16.818572	901.871264	13.740288
17.181679	904.917821	13.745306
17.087881	905.206312	13.750323
16.837820	905.157704	13.755341
17.175448	903.787428	13.760359
16.776304	911.010017	13.765376
17.321854	909.780106	13.770394
17.197471	910.836618	13.775411
16.970311	904.772689	13.780429
16.909894	907.383889	13.785447
16.751771	911.122635	13.790464
16.816055	900.065796	13.795482
16.962251	914.362313	13.800499
16.755753	910.133851	13.805517
17.016213	909.684972	13.810535
16.964809	913.617848	13.815552
16.955556	907.861125	13.820570
17.221953	911.803184	13.825587
16.664582	908.598132	13.830605
17.043821	913.015971	13.835623
17.261031	932.527275	13.840640
17.266644	939.301374	13.845658
17.353897	933.596768	13.850675
17.479084	938.614925	13.855693
17.336801	916.761274	13.860711
17.369728	915.611524	13.865728
17.140518	905.959911	13.870746
17.349548	910.458687	13.875763
17.132482	929.571055	13.880781
17.715328	936.525934	13.885799
17.454419	931.562022	13.890816
17.080945	922.833459	13.895834
17.264163	920.871062	13.900851
17.189362	941.450763	13.905869
17.437465	933.595208	13.910887
17.223298	940.666713	13.915904
17.370909	940.390450	13.920922
17.237061	941.765840	13.925939
17.159771	949.864638	13.930957
17.563316	937.215442	13.935975
17.333161	941.104305	13.940992
17.227931	945.009883	13.946010
17.637196	945.044608	13.951027
17.489040	945.154314	13.956045
17.767700	942.626135	13.961063
17.490367	945.018942	13.966080
17.516067	943.666458	13.971098
18.019135	949.444844	13.976115
17.668958	957.360102	13.981133
17.737384	941.622044	13.986151
17.553803	944.735908	13.991168
17.539605	953.482104	13.996186
17.607657	969.222257	14.001203
17.602899	976.094543	14.006221
17.753237	970.094056	14.011239
17.963534	971.399471	14.016256
17.806762	967.991463	14.021274
17.831956	970.272370	14.026291
17.859228	968.768843	14.031309
18.048209	964.129618	14.036327
17.898633	968.939357	14.041344
17.780699	962.774250	14.046362
18.149307	970.236254	14.051379
17.928153	975.147213	14.056397
18.299042	969.593650	14.061415
18.016365	966.696628	14.066432
18.082488	968.151895	14.071450
18.254434	967.971597	14.076467
18.067920	955.133493	14.081485
18.074552	940.605616	14.086503
17.962115	936.946190	14.091520
18.070595	932.860438	14.096538
17.916296	939.089783	14.101555
18.190019	961.889650	14.106573
18.240248	965.118338	14.111591
18.359013	969.351382	14.116608
18.120163	949.765546	14.121626
18.054691	942.187886	14.126643
18.121919	948.980132	14.131661
18.393081	963.550083	14.136679
18.016101	960.769067	14.141696
18.215338	968.953180	14.146714
17.961402	962.026376	14.151731
17.866816	967.650595	14.156749
18.032892	967.760234	14.161767
18.051635	973.761341	14.166784
18.083954	969.708268	14.171802
18.187850	964.602051	14.176819
18.140478	960.512572	14.181837
18.048901	964.126930	14.186855
17.927392	971.345304	14.191872
17.887934	988.727620	14.196890
18.418230	998.187188	14.201907
18.284331	1000.275555	14.206925
18.645050	997.066877	14.211943
18.325720	1007.638361	14.216960
18.136807	1010.862565	14.221978
18.509023	1002.662027	14.226995
18.128122	1008.689563	14.232013
18.131680	1001.049264	14.237031
18.484451	997.134451	14.242048
18.498998	1003.437433	14.247066
18.620970	997.395178	14.252083
18.687508	1019.573166	14.257101
18.564180	1021.898358	14.262119
18.789899	1024.376374	14.267136
18.846568	1021.034975	14.272154
19.018634	998.367375	14.277171
18.685955	1009.087521	14.282189
18.656649	997.702817	14.287207
18.692453	997.929693	14.292224
18.500692	994.952653	14.297242
19.006205	1005.953669	14.302259
18.818600	1008.150925	14.307277
18.828827	1004.110557	14.312295
18.906166	1001.000376	14.317312
18.542549	997.408118	14.322330
19.030327	1009.149444	14.327347
18.877251	1017.667109	14.332365
18.997933	1016.128819	14.337383
18.843290	1026.064801	14.342400
19.067076	1021.913083	14.347418
19.420410	1013.005458	14.352435
19.257053	1012.243701	14.357453
19.254790	1004.181546	14.362471
18.876480	990.026802	14.367488
18.786598	997.126570	14.372506
19.161019	987.499355	14.377523
18.617418	990.190973	14.382541
18.771087	1001.452601	14.387559
19.093165	1016.636980	14.392576
18.688303	1024.229845	14.397594
19.102252	1020.041126	14.402611
18.653509	1019.229779	14.407629
18.777581	1019.246378	14.412647
18.971428	1014.565783	14.417664
18.867964	1017.388059	14.422682
19.485715	1020.225550	14.427699
19.192720	1017.980594	14.432717
18.919115	1017.908720	14.437735
19.147808	1033.091650	14.442752
19.255800	1045.043130	14.447770
19.279208	1052.580445	14.452787
19.734722	1051.067019	14.457805
19.492771	1042.549671	14.462823
19.545940	1044.511008	14.467840
19.220487	1044.280402	14.472858
19.747570	1042.043736	14.477875
19.239893	1031.094506	14.482893
19.231939	1037.390205	14.487911
19.629675	1050.440124	14.492928
19.330686	1054.728588	14.497946
19.704526	1045.027027	14.502963
19.827662	1054.430041	14.507981
19.420795	1030.320915	14.512999
19.407616	1039.117383	14.518016
19.270099	1051.148103	14.523034
19.690177	1039.587778	14.528051
19.619356	1050.313015	14.533069
19.757780	1047.706863	14.538087
19.918106	1045.058505	14.543104
19.894671	1054.734599	14.548122
20.134987	1031.911559	14.553139
19.595641	1025.603618	14.558157
19.678874	1021.211405	14.563175
19.621808	1019.381301	14.568192
19.668053	1021.955175	14.573210
19.694613	1010.376572	14.578227
19.541821	1019.101269	14.583245
19.590226	1039.435117	14.588263
19.987353	1035.879865	14.593280
19.602599	1053.794216	14.598298
20.003487	1049.321049	14.603315
19.902707	1052.218081	14.608333
19.885518	1050.199093	14.613351
20.275269	1046.349402	14.618368
19.896281	1050.427105	14.623386
20.093209	1040.123763	14.628403
20.154606	1050.652704	14.633421
19.955106	1047.925350	14.638439
20.002684	1044.018151	14.643456
19.824672	1047.294492	14.648474
20.012682	1034.569889	14.653491
19.874531	1044.373629	14.658509
20.005819	1045.569303	14.663527
20.199710	1039.548586	14.668544
20.042993	1047.527127	14.673562
19.923098	1047.199493	14.678579
20.186901	1045.517427	14.683597
20.066178	1047.080410	14.688615
20.097937	1042.282951	14.693632
19.831373	1042.694537	14.698650
20.274382	1041.008386	14.703667
20.370666	1035.007771	14.708685
20.133370	1036.644778	14.713703
20.568538	1037.279128	14.718720
19.737046	1049.763331	14.723738
19.972680	1059.211103	14.728755
20.184278	1062.693395	14.733773
20.010021	1069.839843	14.738791
20.143085	1067.069228	14.743808
20.145623	1078.503176	14.748826
20.537329	1060.217855	14.753843
20.134949	1072.330244	14.758861
20.275610	1069.841037	14.763879
20.395599	1068.397342	14.768896
20.508813	1083.911638	14.773914
20.642480	1091.381109	14.778931
20.565751	1082.693472	14.783949
20.771993	1082.181522	14.788967
20.554414	1079.757540	14.793984
20.835877	1082.231452	14.799002
20.878449	1075.392501	14.804019
20.775535	1066.225368	14.809037
20.684467	1072.571457	14.814055
21.213231	1060.464005	14.819072
20.786798	1074.280708	14.824090
20.663285	1061.587590	14.829107
20.278595	1064.106061	14.834125
20.409849	1067.583942	14.839143
20.762798	1066.274894	14.844160
20.387990	1084.413609	14.849178
20.704355	1096.468415	14.854195
21.040735	1094.769995	14.859213
21.312716	1102.688599	14.864231
21.167998	1087.067575	14.869248
20.814469	1080.612705	14.874266
20.860868	1074.987251	14.879283
21.182098	1075.209776	14.884301
21.276602	1077.006404	14.889319
20.929988	1061.030270	14.894336
20.595457	1073.275907	14.899354
21.151215	1085.279647	14.904371
21.214656	1095.580335	14.909389
21.116146	1088.025396	14.914407
21.231031	1070.733505	14.919424
21.136032	1062.957533	14.924442
21.070480	1059.644238	14.929459
20.929514	1059.689371	14.934477
20.968760	1085.297829	14.939495
21.241012	1090.893630	14.944512
21.451440	1096.468964	14.949530
21.680529	1090.660895	14.954547
21.643725	1070.558790	14.959565
21.183203	1071.650108	14.964583
21.343589	1060.945732	14.969600
21.083478	1056.038731	14.974618
20.951785	1060.836482	14.979635
21.753723	1072.707719	14.984653
21.456676	1087.751784	14.989671
21.420364	1066.584679	14.994688
21.291267	1077.649100	14.999706
21.303849	1090.436070	15.004723
21.495719	1092.259882	15.009741
21.585123	1097.641091	15.014759
21.618050	1096.174409	15.019776
21.684249	1096.560421	15.024794
21.439371	1093.429958	15.029811
21.704539	1091.275630	15.034829
21.576849	1099.888345	15.039847
21.838678	1095.146471	15.044864
21.839165	1081.005293	15.049882
21.346419	1061.764103	15.054899
21.553928	1068.575297	15.059917
21.335022	1084.095378	15.064935
21.698140	1091.282769	15.069952
21.712758	1093.017827	15.074970
21.794448	1094.789808	15.079987
21.636401	1095.220433	15.085005
21.458358	1095.354379	15.090023
21.664544	1092.379532	15.095040
21.756597	1097.570151	15.100058
21.611020	1091.217451	15.105075
21.533887	1086.329352	15.110093
21.369826	1104.157611	15.115111
21.592128	1106.083863	15.120128
21.923934	1113.548488	15.125146
21.981337	1126.943793	15.130163
22.216427	1125.110573	15.135181
21.756464	1139.055717	15.140199
22.006591	1126.867585	15.145216
22.273311	1124.594889	15.150234
22.029935	1129.385171	15.155251
22.101119	1126.998008	15.160269
22.178780	1132.006382	15.165287
22.063604	1123.569962	15.170304
22.426835	1121.347032	15.175322
21.907185	1125.339388	15.180339
22.099593	1124.438402	15.185357
22.012646	1126.451690	15.190375
22.050568	1117.734812	15.195392
22.170772	1126.165947	15.200410
21.868688	1130.993903	15.205427
22.254543	1119.030931	15.210445
21.982095	1125.165746	15.215463
21.903914	1123.775725	15.220480
22.288688	1127.472655	15.225498
22.354309	1138.613927	15.230515
22.612173	1135.100611	15.235533
22.238229	1148.738222	15.240551
22.663557	1146.124702	15.245568
22.444099	1132.520277	15.250586
22.268157	1137.119086	15.255603
22.479256	1141.042015	15.260621
22.305542	1153.099279	15.265639
22.380100	1145.919578	15.270656
22.374626	1146.865081	15.275674
22.359462	1154.843858	15.280691
22.549223	1150.942221	15.285709
22.770947	1152.472130	15.290727
22.579503	1150.281596	15.295744
22.772879	1146.639983	15.300762
22.355298	1153.094107	15.305779
23.039213	1149.077574	15.310797
22.360660	1147.483039	15.315815
22.690564	1151.458343	15.320832
22.821793	1144.777904	15.325850
22.622402	1149.849089	15.330867
22.549338	1149.629837	15.335885
22.731730	1160.718326	15.340903
22.816677	1168.710847	15.345920
23.201224	1173.073160	15.350938
23.037019	1168.172682	15.355955
22.766095	1158.611674	15.360973
22.828655	1159.092776	15.365991
22.709501	1170.705206	15.371008
23.301541	1166.627112	15.376026
22.889283	1175.850360	15.381043
23.275354	1170.575306	15.386061
23.424107	1173.038139	15.391079
23.178403	1160.319898	15.396096
23.333390	1152.698542	15.401114
23.032189	1147.900281	15.406131
23.123274	1138.306505	15.411149
23.159549	1149.931764	15.416167
23.210656	1155.019737	15.421184
23.082640	1165.718699	15.426202
23.325903	1165.207309	15.431219
23.702144	1166.541559	15.436237
23.375287	1165.876551	15.441255
23.143826	1153.886250	15.446272
23.428443	1138.203924	15.451290
22.963753	1165.043561	15.456307
23.326034	1152.470313	15.461325
23.191490	1168.597749	15.466343
23.677420	1168.817412	15.471360
23.654336	1174.136174	15.476378
23.414637	1166.660874	15.481395
23.443702	1168.814007	15.486413
23.472608	1168.660543	15.491431
23.605135	1167.025005	15.496448
23.463367	1164.460113	15.501466
23.562777	1174.758834	15.506483
23.875722	1166.190477	15.511501
24.030947	1168.409331	15.516519
23.689958	1165.571532	15.521536
24.030502	1167.453016	15.526554
23.737477	1155.045362	15.531571
23.790443	1147.755459	15.536589
23.699823	1147.046215	15.541607
23.862145	1144.247908	15.546624
23.826499	1139.599765	15.551642
23.501363	1135.051526	15.556659
23.840276	1141.952407	15.561677
23.867274	1159.986095	15.566695
23.916527	1167.565248	15.571712
24.276200	1159.585202	15.576730
23.879913	1156.716404	15.581747
23.922940	1139.628062	15.586765
23.914867	1147.060403	15.591783
23.591740	1170.383018	15.596800
24.078987	1158.092213	15.601818
23.991193	1173.498155	15.606835
23.697587	1169.617894	15.611853
23.820330	1169.742190	15.616871
23.951947	1165.343106	15.621888
24.339612	1167.536069	15.626906
23.984735	1175.224270	15.631923
24.126352	1162.685191	15.636941
24.148908	1166.733439	15.641959
23.880835	1178.027237	15.646976
24.194964	1155.236674	15.651994
24.313664	1161.804355	15.657011
24.178389	1160.554097	15.662029
23.986397	1163.017054	15.667047
24.167103	1179.848576	15.672064
24.523159	1188.503675	15.677082
24.625899	1197.264896	15.682099
24.576919	1186.047874	15.687117
24.708693	1170.896715	15.692135
24.344383	1163.873926	15.697152
24.632143	1159.048213	15.702170
23.857044	1154.578414	15.707187
24.346562	1179.958143	15.712205
24.589127	1185.607319	15.717223
24.741719	1188.947840	15.722240
24.999981	1189.298508	15.727258
24.717914	1180.999137	15.732275
25.139250	1184.123508	15.737293
24.715670	1172.252798	15.742311
24.499044	1163.915042	15.747328
24.710660	1156.222892	15.752346
24.474870	1168.635712	15.757363
24.743686	1174.665959	15.762381
25.092419	1187.726077	15.767399
24.874040	1186.505325	15.772416
24.954247	1185.746533	15.777434
25.149522	1194.209367	15.782451
24.624410	1160.574222	15.787469
24.626381	1171.591811	15.792487
24.456319	1181.937520	15.797504
24.768784	1175.055016	15.802522
24.962416	1184.732648	15.807539
24.796604	1182.582352	15.812557
25.081421	1188.271381	15.817575
24.810388	1187.793973	15.822592
24.970552	1178.386759	15.827610
24.678527	1181.033602	15.832627
24.819651	1189.639255	15.837645
25.044321	1191.169861	15.842663
24.890764	1214.432574	15.847680
25.350644	1214.929380	15.852698
25.078210	1217.848173	15.857715
24.989747	1214.826033	15.862733
25.371999	1220.124935	15.867751
25.134137	1219.103070	15.872768
25.591779	1213.750404	15.877786
25.102801	1222.247426	15.882803
25.245106	1219.184317	15.887821
25.300373	1208.727948	15.892839
25.168069	1215.403749	15.897856
25.370836	1220.802054	15.902874
25.363079	1217.239005	15.907891
25.572305	1219.225309	15.912909
25.515024	1210.707209	15.917927
25.235826	1216.544366	15.922944
25.430431	1218.055938	15.927962
25.352518	1213.071080	15.932979
25.589731	1219.183741	15.937997
25.551710	1213.989527	15.943015
25.418966	1221.012244	15.948032
26.026790	1232.233088	15.953050
26.137911	1230.528255	15.958067
25.644949	1219.882745	15.963085
25.599453	1214.222852	15.968103
25.744653	1214.104460	15.973120
25.760568	1213.555127	15.978138
25.826208	1228.812886	15.983155
25.975584	1232.885032	15.988173
26.379109	1225.394135	15.993191
25.886892	1221.904218	15.998208
25.809949	1204.614023	16.003226
25.714760	1221.661743	16.008243
26.125447	1233.276246	16.013261
26.276971	1221.027992	16.018279
25.931518	1215.705949	16.023296
25.753268	1208.816106	16.028314
25.917741	1225.070854	16.033331
26.102864	1236.488858	16.038349
26.083545	1235.784338	16.043367
25.861987	1235.871949	16.048384
25.953433	1240.393442	16.053402
26.205700	1236.127506	16.058419
25.999993	1238.650224	16.063437
26.112533	1228.739462	16.068455
26.233829	1244.124237	16.073472
26.462013	1240.653606	16.078490
26.243660	1241.621372	16.083507
26.233049	1243.657861	16.088525
26.618025	1234.953132	16.093543
26.360149	1245.450823	16.098560
26.230020	1237.357360	16.103578
26.568669	1234.786131	16.108595
26.232113	1237.017139	16.113613
26.225969	1234.197500	16.118631
26.329379	1257.242534	16.123648
26.676745	1266.004625	16.128666
26.698924	1267.438457	16.133683
26.783807	1266.288345	16.138701
26.798584	1261.408593	16.143719
26.878098	1263.295125	16.148736
26.666844	1249.681757	16.153754
26.598658	1242.068967	16.158771
26.760713	1255.295877	16.163789
26.891363	1251.091019	16.168807
26.677832	1252.082790	16.173824
26.818532	1251.133667	16.178842
27.140306	1256.605190	16.183859
26.866288	1253.952736	16.188877
27.044835	1240.279161	16.193895
26.552298	1240.776200	16.198912
27.140772	1255.825366	16.203930
27.290717	1245.651319	16.208947
26.594341	1247.771049	16.213965
27.295260	1245.742572	16.218983
27.274208	1250.851974	16.224000
26.944607	1239.992002	16.229018
26.934395	1236.006530	16.234035
27.030196	1259.107157	16.239053
27.208434	1250.364214	16.244071
26.998127	1252.207005	16.249088
27.270461	1253.869092	16.254106
27.232321	1249.491794	16.259123
26.955087	1264.778806	16.264141
27.262566	1257.171124	16.269159
27.131520	1260.025963	16.274176
27.137671	1250.050916	16.279194
27.429127	1254.291663	16.284211
27.252421	1251.435698	16.289229
27.085040	1251.021831	16.294247
27.399292	1259.604760	16.299264
27.449145	1255.758940	16.304282
27.541089	1258.889052	16.309299
27.303516	1252.008225	16.314317
27.372027	1247.937276	16.319335
27.518319	1263.057307	16.324352
27.354797	1265.721073	16.329370
27.692260	1277.698120	16.334387
27.469266	1285.696419	16.339405
27.754316	1277.017268	16.344423
27.533509	1282.657384	16.349440
27.942322	1281.820946	16.354458
28.341566	1286.559590	16.359475
28.166852	1281.320666	16.364493
28.188143	1258.922528	16.369511
28.047788	1249.748494	16.374528
27.765950	1244.601336	16.379546
27.940082	1240.166845	16.384563
27.914279	1250.243443	16.389581
28.111266	1246.238620	16.394599
27.872235	1244.751604	16.399616
27.757620	1240.557834	16.404634
27.979519	1242.788100	16.409651
27.980741	1251.753165	16.414669
27.758367	1258.173827	16.419687
27.718708	1270.440475	16.424704
27.703724	1280.696006	16.429722
28.036831	1277.602866	16.434739
27.774042	1285.980186	16.439757
27.713131	1280.092118	16.444775
28.156007	1279.274450	16.449792
28.056459	1291.452214	16.454810
28.235501	1306.988904	16.459827
28.469714	1309.683272	16.464845
28.487768	1303.027017	16.469863
28.411088	1305.094532	16.474880
28.130549	1301.164436	16.479898
28.705862	1295.051329	16.484915
28.462276	1307.476969	16.489933
28.490807	1300.560718	16.494951
28.434977	1295.579263	16.499968
28.570943	1298.937128	16.504986
28.751884	1298.212437	16.510003
28.389532	1301.914622	16.515021
28.689363	1291.557462	16.520039
28.652603	1298.473771	16.525056
28.552568	1292.586271	16.530074
28.971904	1288.556429	16.535091
28.666721	1299.019471	16.540109
29.095709	1294.708115	16.545127
28.876403	1292.334383	16.550144
28.605852	1300.040570	16.555162
29.003662	1298.988636	16.560179
28.691076	1296.764599	16.565197
28.732199	1298.815756	16.570215
28.791101	1299.745096	16.575232
28.725716	1290.754682	16.580250
29.026265	1295.881710	16.585267
28.805578	1301.656455	16.590285
28.890003	1300.565471	16.595303
28.768074	1297.254768	16.600320
28.870849	1299.910664	16.605338
29.219756	1302.521473	16.610355
29.064898	1307.032984	16.615373
29.060880	1315.014723	16.620391
29.561846	1319.886923	16.625408
29.136942	1314.146121	16.630426
29.188320	1316.595574	16.635443
29.627684	1317.918205	16.640461
29.587842	1314.845870	16.645479
29.486779	1294.260030	16.650496
29.246800	1297.075041	16.655514
29.516571	1284.778810	16.660531
29.421697	1293.377931	16.665549
29.357077	1287.053870	16.670567
29.401610	1303.379741	16.675584
29.601768	1320.069615	16.680602
29.272480	1318.608954	16.685619
29.247463	1321.119483	16.690637
29.576100	1330.222106	16.695655
29.480086	1328.438571	16.700672
29.186347	1317.097026	16.705690
29.524136	1314.564115	16.710707
29.565730	1326.419330	16.715725
29.327660	1321.242851	16.720743
29.578862	1331.345285	16.725760
29.835959	1341.756981	16.730778
30.171813	1351.081252	16.735795
30.169761	1350.348278	16.740813
30.286748	1338.483596	16.745831
30.318444	1323.904754	16.750848
30.019676	1317.313159	16.755866
30.161693	1317.880713	16.760883
30.413835	1316.998958	16.765901
30.508743	1317.553841	16.770919
30.210955	1314.576185	16.775936
30.184584	1309.256784	16.780954
30.410105	1309.828226	16.785971
30.451907	1310.533632	16.790989
30.293791	1310.419009	16.796007
30.386587	1309.711275	16.801024
30.255511	1314.840491	16.806042
30.413226	1310.426415	16.811059
30.063454	1312.910010	16.816077
30.173527	1309.609706	16.821095
30.624645	1315.436990	16.826112
30.095626	1316.696356	16.831130
30.485559	1308.778938	16.836147
30.274279	1310.497096	16.841165
30.167852	1305.686612	16.846183
30.452833	1305.722629	16.851200
30.174796	1308.195920	16.856218
30.094108	1310.917629	16.861235
30.544309	1313.671900	16.866253
30.232338	1317.841722	16.871271
30.400316	1332.297220	16.876288
30.504319	1349.029818	16.881306
30.578597	1344.829545	16.886323
30.715233	1339.208344	16.891341
30.607068	1339.580716	16.896359
30.665383	1339.486553	16.901376
30.393316	1346.936326	16.906394
30.466654	1335.873347	16.911411
30.530093	1347.775747	16.916429
30.668455	1357.387838	16.921447
31.642730	1362.219473	16.926464
31.544674	1350.142757	16.931482
31.675058	1328.180777	16.936499
31.572480	1325.823931	16.941517
31.101121	1324.172232	16.946535
31.455533	1314.942216	16.951552
31.423842	1322.783662	16.956570
31.419933	1324.225757	16.961587
31.546531	1316.605478	16.966605
31.295376	1306.072227	16.971623
31.511804	1290.464422	16.976640
31.130063	1287.521932	16.981658
31.375467	1287.609778	16.986675
31.206040	1288.378111	16.991693
31.155324	1311.021198	16.996711
31.733215	1313.127960	17.001728
31.420795	1316.381339	17.006746
31.319859	1322.690976	17.011763
31.562691	1321.575728	17.016781
31.348038	1320.115376	17.021799
31.435485	1311.898052	17.026816
31.222058	1319.415660	17.031834
31.318903	1323.410310	17.036851
31.827912	1319.611277	17.041869
31.171183	1318.360738	17.046887
31.463891	1319.121446	17.051904
31.600128	1318.568720	17.056922
31.423638	1323.981831	17.061939
31.476860	1329.374623	17.066957
31.546551	1349.334889	17.071975
31.675827	1351.041541	17.076992
31.658869	1356.000695	17.082010
31.560900	1350.485266	17.087027
32.016612	1358.281061	17.092045
31.683176	1359.593869	17.097063
32.044700	1350.425251	17.102080
31.971850	1355.931447	17.107098
31.982449	1360.251406	17.112115
32.186080	1362.760299	17.117133
32.261400	1368.454559	17.122151
32.404330	1371.465623	17.127168
32.311412	1370.087469	17.132186
32.069997	1370.929536	17.137203
32.439044	1361.201015	17.142221
32.527818	1366.271009	17.147239
32.361105	1361.968906	17.152256
32.119440	1358.091019	17.157274
32.252249	1360.819116	17.162291
32.357307	1364.800606	17.167309
32.493304	1372.897771	17.172327
32.508011	1368.124687	17.177344
32.565611	1376.126963	17.182362
32.689697	1374.862479	17.187379
32.679991	1370.109186	17.192397
32.564355	1378.931079	17.197415
32.730478	1371.024313	17.202432
32.551858	1368.826900	17.207450
32.370445	1362.257191	17.212467
32.939880	1370.488878	17.217485
32.585551	1370.308715	17.222503
32.887222	1375.021812	17.227520
32.595171	1370.675895	17.232538
32.786702	1370.802189	17.237555
32.758997	1370.373063	17.242573
32.846997	1368.966132	17.247591
32.967637	1358.900799	17.252608
32.807997	1369.059871	17.257626
32.816806	1360.475234	17.262643
32.714454	1362.874168	17.267661
32.938388	1389.758037	17.272679
33.079486	1393.951280	17.277696
32.774391	1404.269104	17.282714
33.061332	1401.023350	17.287731
33.535857	1394.981224	17.292749
33.219794	1399.607249	17.297767
33.379408	1388.812619	17.302784
33.547215	1392.697113	17.307802
33.586392	1393.874997	17.312819
33.630963	1384.329322	17.317837
33.246838	1390.728791	17.322855
33.561378	1390.287481	17.327872
33.512377	1392.484281	17.332890
33.668871	1388.968402	17.337907
33.750276	1384.807095	17.342925
33.554527	1389.120286	17.347943
33.637092	1392.124420	17.352960
33.665273	1380.004731	17.357978
33.712978	1392.482596	17.362995
33.778397	1394.693914	17.368013
33.706709	1396.844865	17.373031
34.019507	1382.790278	17.378048
33.984377	1392.972843	17.383066
33.759547	1386.529208	17.388083
33.881415	1388.946135	17.393101
33.810263	1396.021330	17.398119
33.939597	1392.543806	17.403136
33.894078	1402.212357	17.408154
34.088812	1391.432382	17.413171
33.939491	1389.780893	17.418189
33.935537	1393.839889	17.423207
34.330794	1389.662437	17.428224
34.400312	1393.950996	17.433242
34.010505	1396.527058	17.438259
34.335766	1381.756247	17.443277
34.274692	1390.771865	17.448295
34.140251	1389.839161	17.453312
34.204656	1391.356168	17.458330
34.221544	1400.171090	17.463347
34.539722	1397.726452	17.468365
34.163272	1396.636186	17.473383
34.183076	1390.196530	17.478400
34.068308	1393.558532	17.483418
33.787626	1401.622741	17.488435
34.463891	1407.991511	17.493453
34.281494	1418.526819	17.498471
34.464012	1416.058579	17.503488
34.810800	1417.752844	17.508506
34.480927	1420.033163	17.513523
34.969076	1410.883700	17.518541
34.780557	1422.406624	17.523559
34.535666	1418.948541	17.528576
34.920995	1419.935253	17.533594
34.479854	1417.742720	17.538611
34.825911	1407.477433	17.543629
34.844837	1415.435740	17.548647
34.790001	1423.923187	17.553664
34.737284	1416.451841	17.558682
34.692844	1443.928268	17.563699
34.955884	1442.161248	17.568717
34.692158	1453.217127	17.573735
35.056931	1447.104573	17.578752
35.277589	1448.679964	17.583770
35.284662	1448.780110	17.588787
35.489585	1433.081943	17.593805
35.427173	1449.224498	17.598823
35.658481	1439.762433	17.603840
35.547571	1440.146679	17.608858
35.418075	1440.643450	17.613875
35.743694	1435.852328	17.618893
35.393430	1423.448817	17.623911
34.962722	1424.887184	17.628928
35.498942	1426.088671	17.633946
35.113288	1430.016789	17.638963
35.860636	1426.855815	17.643981
35.509151	1436.700246	17.648999
35.461848	1437.279075	17.654016
35.718590	1434.221384	17.659034
35.730937	1431.111249	17.664051
35.446989	1428.823002	17.669069
35.518529	1436.104112	17.674087
35.950367	1431.324536	17.679104
36.055267	1434.911981	17.684122
35.892238	1431.397427	17.689139
36.029764	1428.895297	17.694157
36.408599	1427.615792	17.699175
35.760433	1424.200862	17.704192
36.077103	1426.594987	17.709210
36.019575	1424.181061	17.714227
35.593857	1426.661895	17.719245
35.372885	1430.943054	17.724263
35.849453	1436.156730	17.729280
35.874354	1450.041156	17.734298
36.083306	1453.737752	17.739315
36.087119	1450.492021	17.744333
36.091665	1454.740174	17.749351
35.711988	1459.810210	17.754368
36.294333	1459.334790	17.759386
36.128691	1468.065409	17.764403
36.369087	1485.312573	17.769421
36.395092	1496.248854	17.774439
36.645809	1488.298493	17.779456
36.396068	1489.953355	17.784474
36.600413	1486.607088	17.789491
36.874684	1487.907467	17.794509
36.395332	1486.870060	17.799527
36.791184	1481.799973	17.804544
36.986102	1488.913042	17.809562
36.915385	1495.963407	17.814579
36.887129	1485.850994	17.819597
37.050815	1479.410704	17.824615
37.105123	1482.841973	17.829632
37.376790	1478.208982	17.834650
36.966771	1461.360263	17.839667
37.076853	1445.304170	17.844685
36.934888	1449.074226	17.849703
36.649994	1456.502160	17.854720
37.168857	1462.338362	17.859738
36.805518	1472.608789	17.864755
37.118793	1477.918415	17.869773
37.122717	1478.329316	17.874791
37.290010	1484.590273	17.879808
37.315852	1476.332669	17.884826
37.210544	1482.251367	17.889843
37.406761	1476.879303	17.894861
37.383486	1477.704546	17.899879
37.030818	1475.949318	17.904896
37.557089	1471.837945	17.909914
37.080815	1475.375966	17.914931
37.226100	1466.219858	17.919949
37.586597	1475.837366	17.924967
37.043337	1471.231052	17.929984
37.104668	1479.320163	17.935002
37.294469	1490.044280	17.940019
37.577171	1500.880974	17.945037
37.939394	1504.059687	17.950055
37.500492	1504.517537	17.955072
37.820555	1501.774935	17.960090
37.838304	1500.680017	17.965107
38.014578	1499.391134	17.970125
37.906427	1502.285139	17.975143
37.720546	1498.970809	17.980160
38.317798	1489.305207	17.985178
37.894760	1498.553657	17.990195
37.612295	1494.650208	17.995213
37.762434	1503.955324	18.000231
37.871248	1515.955064	18.005248
38.385092	1518.884267	18.010266
38.366774	1523.353546	18.015283
38.718305	1518.511258	18.020301
38.655726	1507.495072	18.025319
38.362874	1497.017019	18.030336
38.263340	1487.173098	18.035354
38.301134	1500.327488	18.040371
38.329475	1491.153329	18.045389
38.537188	1501.191818	18.050407
38.590110	1514.692925	18.055424
38.649668	1513.357620	18.060442
38.414447	1511.493571	18.065459
38.724866	1526.234324	18.070477
38.698502	1524.728601	18.075495
38.507433	1530.230024	18.080512
38.893236	1517.125426	18.085530
38.725325	1528.653679	18.090547
38.364803	1522.858436	18.095565
38.388369	1515.817715	18.100583
38.199735	1528.148605	18.105600
38.704491	1523.492753	18.110618
38.689976	1540.368411	18.115635
38.885643	1541.887320	18.120653
39.279568	1546.438345	18.125671
39.110839	1549.642781	18.130688
39.546552	1546.656614	18.135706
39.186220	1547.901450	18.140723
39.518384	1550.095392	18.145741
39.286413	1530.875001	18.150759
39.287075	1538.778916	18.155776
39.725984	1534.455222	18.160794
39.374289	1528.350643	18.165811
39.035029	1515.516498	18.170829
39.535610	1517.829005	18.175847
39.294277	1536.379212	18.180864
39.368815	1543.264603	18.185882
39.262402	1538.743018	18.190899
39.522980	1541.034638	18.195917
39.773717	1537.840521	18.200935
39.656220	1541.189228	18.205952
39.718323	1537.273987	18.210970
39.589702	1548.870158	18.215987
39.604840	1543.126876	18.221005
39.691797	1535.338253	18.226023
39.564158	1544.490178	18.231040
39.998099	1546.101916	18.236058
39.834188	1539.774508	18.241075
39.701444	1540.408039	18.246093
40.091850	1539.139208	18.251111
39.789620	1544.139754	18.256128
39.967865	1544.648956	18.261146
39.987413	1560.589080	18.266163
40.100383	1572.031485	18.271181
40.352520	1560.024570	18.276199
39.903909	1572.315079	18.281216
40.206361	1568.214758	18.286234
40.305260	1567.830410	18.291251
40.507388	1564.982130	18.296269
40.758476	1565.720609	18.301287
40.316205	1568.403811	18.306304
40.245575	1561.296777	18.311322
40.367743	1557.848355	18.316339
40.361260	1565.102682	18.321357
40.611131	1558.441396	18.326375
40.151856	1566.171878	18.331392
40.657614	1564.151270	18.336410
40.978993	1564.841496	18.341427
40.166137	1568.382120	18.346445
41.180855	1565.883931	18.351463
40.727964	1563.938990	18.356480
40.657273	1559.157155	18.361498
41.067462	1569.350349	18.366515
40.884175	1585.367785	18.371533
41.376968	1580.045002	18.376551
41.127070	1585.115242	18.381568
41.297330	1568.401815	18.386586
41.092052	1552.080116	18.391603
41.095476	1557.711153	18.396621
41.174462	1558.176162	18.401639
41.067034	1571.445210	18.406656
41.203959	1583.565150	18.411674
41.288114	1582.254113	18.416691
41.554783	1582.016788	18.421709
42.064805	1573.540771	18.426727
41.878187	1557.631328	18.431744
41.906349	1541.078861	18.436762
42.041811	1542.349080	18.441779
41.889706	1540.441738	18.446797
41.788727	1534.058635	18.451815
41.364749	1543.761595	18.456832
41.726554	1539.618383	18.461850
41.779686	1545.789607	18.466867
41.389913	1539.682668	18.471885
41.768369	1538.676837	18.476903
41.518751	1539.815939	18.481920
41.493997	1539.056400	18.486938
42.076233	1552.162415	18.491955
41.483619	1563.349209	18.496973
41.848386	1569.060575	18.501991
41.741216	1576.837876	18.507008
41.722732	1570.084407	18.512026
42.193198	1576.284965	18.517043
42.033213	1584.723375	18.522061
42.194483	1568.245688	18.527079
41.924402	1584.132614	18.532096
42.155790	1588.267652	18.537114
42.614502	1593.473316	18.542131
41.960661	1591.610071	18.547149
42.380948	1594.794150	18.552167
42.516669	1603.960376	18.557184
42.339556	1611.576836	18.562202
42.126033	1599.459202	18.567219
42.165607	1611.511819	18.572237
42.551852	1603.487384	18.577255
42.398011	1598.154345	18.582272
42.693893	1600.828711	18.587290
43.014591	1606.062743	18.592307
42.931754	1607.569508	18.597325
43.083784	1599.356692	18.602343
42.959708	1597.050608	18.607360
43.047138	1599.703585	18.612378
43.265952	1592.933255	18.617395
43.117821	1606.038994	18.622413
43.122579	1603.273782	18.627431
42.709631	1599.446635	18.632448
42.968009	1606.993344	18.637466
43.194651	1599.835495	18.642483
42.971799	1592.607196	18.647501
43.040910	1601.023429	18.652519
43.116251	1600.319754	18.657536
43.234045	1615.612566	18.662554
43.601228	1619.261742	18.667571
43.458680	1627.414217	18.672589
43.983954	1621.017539	18.677607
43.605654	1603.575617	18.682624
43.119548	1597.763345	18.687642
43.567780	1598.134143	18.692659
43.600192	1618.171006	18.697677
43.866233	1613.790482	18.702695
43.977236	1614.511608	18.707712
44.062057	1610.918965	18.712730
43.655005	1602.618014	18.717747
43.619019	1609.314256	18.722765
44.071808	1605.651236	18.727783
44.097033	1607.253886	18.732800
44.044769	1609.928815	18.737818
44.167954	1611.316427	18.742835
43.869623	1619.643118	18.747853
43.894349	1609.891142	18.752871
43.965285	1614.905117	18.757888
43.777147	1616.594673	18.762906
44.041346	1611.179810	18.767923
44.094659	1616.760483	18.772941
43.864632	1621.994767	18.777959
43.775221	1625.812856	18.782976
44.168542	1643.726213	18.787994
44.556980	1634.936832	18.793011
44.198360	1646.001080	18.798029
44.288865	1645.907885	18.803047
44.633466	1653.179315	18.808064
44.673343	1649.793712	18.813082
44.617956	1636.163642	18.818099
44.241658	1665.407223	18.823117
44.506097	1660.268288	18.828135
44.811155	1665.299418	18.833152
44.753469	1674.913854	18.838170
45.369572	1672.741104	18.843187
45.426469	1675.759780	18.848205
45.320306	1656.828638	18.853223
44.974760	1649.039526	18.858240
45.090668	1642.329520	18.863258
45.385743	1634.122922	18.868275
45.199607	1640.425535	18.873293
44.939373	1639.473487	18.878311
45.016085	1631.593205	18.883328
44.926796	1658.491611	18.888346
45.607526	1669.636533	18.893363
45.206877	1667.246706	18.898381
45.327236	1667.180851	18.903399
45.243255	1670.738209	18.908416
45.206221	1673.284249	18.913434
45.794029	1664.261444	18.918451
45.285583	1673.802486	18.923469
45.218843	1668.447913	18.928487
45.517778	1666.503272	18.933504
45.528720	1668.393728	18.938522
46.039875	1676.704917	18.943539
45.371254	1680.959086	18.948557
45.602269	1688.855643	18.953575
46.067597	1692.019292	18.958592
45.744347	1700.805667	18.963610
46.294089	1695.276958	18.968627
46.406793	1690.872590	18.973645
46.403974	1694.170451	18.978663
46.506455	1691.869358	18.983680
46.074360	1683.254792	18.988698
46.064146	1666.520356	18.993715
45.786264	1675.731489	18.998733
46.065623	1685.281855	19.003751
46.222129	1689.733258	19.008768
45.970158	1690.282993	19.013786
46.303530	1685.887364	19.018803
46.092788	1693.772031	19.023821
46.448294	1687.711705	19.028839
46.503749	1696.421984	19.033856
46.596748	1704.982744	19.038874
46.835033	1712.384012	19.043891
47.017736	1709.335378	19.048909
47.007458	1703.853727	19.053927
46.902327	1683.677099	19.058944
46.357694	1690.987523	19.063962
46.811679	1702.415290	19.068979
46.597429	1709.877710	19.073997
46.540676	1705.965966	19.079015
46.863088	1700.327653	19.084032
46.677484	1710.283372	19.089050
47.067629	1705.608256	19.094067
47.220873	1716.279135	19.099085
47.410776	1722.402979	19.104103
47.451026	1723.234646	19.109120
47.300805	1708.584383	19.114138
47.589916	1717.385906	19.119155
47.701813	1707.195416	19.124173
47.590423	1700.006879	19.129191
47.708313	1697.309531	19.134208
47.572664	1700.741593	19.139226
47.584900	1693.977472	19.144243
47.766744	1698.925866	19.149261
47.701392	1691.466716	19.154279
47.906432	1690.275023	19.159296
47.489417	1701.835596	19.164314
47.765966	1712.460465	19.169331
47.948213	1732.417547	19.174349
47.623597	1718.087492	19.179367
48.022071	1713.226742	19.184384
47.905829	1727.094629	19.189402
48.327789	1719.480365	19.194419
47.997953	1723.259155	19.199437
48.075943	1727.787350	19.204455
48.313726	1719.695705	19.209472
47.825154	1733.855567	19.214490
48.253515	1722.278405	19.219507
48.455466	1725.449846	19.224525
48.462299	1728.146900	19.229543
48.423611	1713.117532	19.234560
48.324572	1730.563301	19.239578
48.430390	1725.121081	19.244595
47.966263	1731.247319	19.249613
48.450957	1749.701185	19.254631
49.009895	1749.695387	19.259648
48.741519	1759.159327	19.264666
48.849527	1749.441898	19.269683
48.854655	1756.953449	19.274701
48.903097	1757.167221	19.279719
49.189584	1751.780903	19.284736
48.919374	1755.417542	19.289754
48.951125	1747.451338	19.294771
49.173614	1747.554794	19.299789
48.680358	1755.419735	19.304807
49.048310	1748.678974	19.309824
48.821549	1754.056070	19.314842
48.779222	1752.508873	19.319859
48.828314	1751.100477	19.324877
49.184607	1771.586669	19.329895
49.382908	1768.495677	19.334912
49.095000	1776.316391	19.339930
49.725544	1777.147956	19.344947
49.968204	1774.419700	19.349965
49.610056	1777.741375	19.354983
49.739510	1777.286608	19.360000
49.697895	1781.355092	19.365018
49.777718	1775.456524	19.370035
49.909128	1767.258451	19.375053
49.910578	1769.823725	19.380071
49.845622	1765.588912	19.385088
49.398189	1768.408042	19.390106
49.587116	1768.045397	19.395123
49.919776	1774.299957	19.400141
49.627954	1769.881446	19.405159
50.082772	1788.029672	19.410176
49.998065	1804.795585	19.415194
50.171020	1798.674105	19.420211
50.283079	1801.307684	19.425229
50.203372	1805.079722	19.430247
50.577450	1797.349726	19.435264
50.350121	1796.252060	19.440282
50.210430	1791.460711	19.445299
50.701326	1792.560679	19.450317
50.650117	1794.270100	19.455335
50.356476	1785.593969	19.460352
50.575502	1789.034251	19.465370
50.669059	1791.333094	19.470387
50.869572	1799.556415	19.475405
50.828072	1812.055295	19.480423
51.010455	1811.092151	19.485440
51.266174	1814.718886	19.490458
50.893289	1803.071185	19.495475
50.934742	1792.519072	19.500493
51.141496	1807.860336	19.505511
51.515775	1806.203206	19.510528
51.187778	1808.460434	19.515546
51.354675	1809.924292	19.520563
51.796986	1803.044815	19.525581
51.455123	1784.872630	19.530599
51.131679	1766.524975	19.535616
51.426528	1785.130792	19.540634
51.384882	1794.981625	19.545651
51.663375	1800.440432	19.550669
51.623264	1811.153235	19.555687
51.768937	1804.614218	19.560704
51.732178	1805.785809	19.565722
51.715576	1796.815763	19.570739
51.701851	1798.467797	19.575757
51.755072	1804.509975	19.580775
51.895939	1800.790684	19.585792
51.963423	1801.796587	19.590810
51.910910	1809.626373	19.595827
52.020918	1798.475889	19.600845
51.750255	1794.185364	19.605863
51.868472	1799.921893	19.610880
51.597965	1798.901062	19.615898
51.594993	1821.235016	19.620915
52.314686	1827.253856	19.625933
51.909917	1839.049907	19.630951
51.874148	1838.403990	19.635968
52.176168	1835.945818	19.640986
52.095749	1838.564818	19.646003
52.354612	1858.147954	19.651021
52.384074	1873.414701	19.656039
52.757751	1866.936331	19.661056
52.660785	1856.055907	19.666074
52.756814	1864.811532	19.671091
53.329040	1864.456679	19.676109
52.960219	1863.857247	19.681127
52.823521	1853.890110	19.686144
53.005199	1856.549967	19.691162
53.130070	1865.273650	19.696179
53.156433	1851.768046	19.701197
52.968950	1858.186326	19.706215
53.101131	1848.503810	19.711232
53.137484	1862.254423	19.716250
52.890061	1860.359674	19.721267
53.344858	1852.098561	19.726285
53.114718	1858.761703	19.731303
53.230980	1849.612145	19.736320
53.548562	1864.059905	19.741338
53.478108	1871.978127	19.746355
53.480920	1875.986522	19.751373
53.516404	1883.723032	19.756391
53.931155	1868.883791	19.761408
53.995666	1869.614203	19.766426
53.520719	1867.885475	19.771443
53.752002	1868.379214	19.776461
53.737971	1870.813995	19.781479
53.753265	1872.484854	19.786496
53.787019	1864.674560	19.791514
54.106813	1870.991526	19.796531
54.339468	1865.582586	19.801549
54.177352	1869.264347	19.806567
54.014316	1868.283984	19.811584
54.163902	1870.481434	19.816602
54.280051	1890.190605	19.821619
54.661028	1892.421399	19.826637
54.480611	1894.823890	19.831655
54.667700	1897.574592	19.836672
54.922961	1892.659153	19.841690
54.754102	1893.806560	19.846707
54.866051	1893.425556	19.851725
55.019735	1887.820626	19.856743
54.564451	1879.246011	19.861760
54.709416	1873.144884	19.866778
54.377468	1885.204507	19.871795
54.728040	1886.646226	19.876813
54.958525	1897.276487	19.881831
54.880705	1894.998920	19.886848
54.928715	1886.944518	19.891866
55.191267	1894.570206	19.896883
54.943550	1889.930181	19.901901
55.065709	1894.796392	19.906919
55.107959	1912.363855	19.911936
55.296090	1918.955009	19.916954
55.441559	1924.522502	19.921971
55.728271	1920.406585	19.926989
55.663130	1920.593103	19.932007
55.138897	1929.463279	19.937024
55.453901	1917.224416	19.942042
55.397974	1928.948993	19.947059
55.556330	1921.047958	19.952077
55.214245	1920.732291	19.957095
55.475812	1919.013496	19.962112
55.408231	1931.184500	19.967130
55.732359	1946.558043	19.972147
55.759257	1943.716662	19.977165
55.929361	1947.660366	19.982183
56.078072	1946.724050	19.987200
56.072789	1945.465982	19.992218
56.137005	1942.501884	19.997235
56.326498	1942.249774	20.002253
56.577982	1938.597569	20.007271
56.685276	1940.489034	20.012288
56.692158	1925.581051	20.017306
56.751778	1935.955373	20.022323
56.722061	1933.149747	20.027341
56.726746	1928.582879	20.032359
56.684499	1932.330241	20.037376
56.761388	1935.664562	20.042394
56.591270	1939.354750	20.047411
56.837259	1924.585921	20.052429
56.772524	1931.167374	20.057447
56.628619	1937.216259	20.062464
57.100859	1946.528546	20.067482
56.817236	1956.124660	20.072499
57.243164	1955.600326	20.077517
57.346322	1955.470388	20.082535
57.238432	1956.995114	20.087552
57.490865	1953.182115	20.092570
57.442362	1956.845477	20.097587
57.554761	1954.829324	20.102605
57.662296	1956.675080	20.107623
57.527783	1959.966063	20.112640
57.487700	1954.060903	20.117658
57.499819	1961.498953	20.122675
57.662934	1959.459440	20.127693
57.560434	1955.046536	20.132711
57.584064	1966.400480	20.137728
57.818524	1957.308061	20.142746
57.579760	1957.904437	20.147763
57.715365	1975.870302	20.152781
57.835229	1984.218890	20.157799
58.074386	1985.222758	20.162816
58.419608	1984.263744	20.167834
58.111489	1989.531948	20.172851
58.215438	1989.481014	20.177869
58.451183	1985.136507	20.182887
58.304138	1990.521350	20.187904
58.338849	1973.292913	20.192922
57.927117	1978.403856	20.197939
58.211604	1987.547646	20.202957
58.644981	2004.748868	20.207975
58.634855	2010.827994	20.212992
59.110402	2002.706677	20.218010
58.476020	2012.063653	20.223027
58.732202	2012.136729	20.228045
58.810263	2014.652743	20.233063
58.759141	2006.346576	20.238080
59.019867	2007.185847	20.243098
58.619679	2009.785380	20.248115
59.089117	2001.038288	20.253133
59.087142	2006.881018	20.258151
59.004963	2025.867671	20.263168
59.625305	2031.694377	20.268186
59.519813	2028.944194	20.273203
59.585740	2026.894781	20.278221
59.797829	2030.026416	20.283239
59.625511	2009.951042	20.288256
60.037516	1993.555801	20.293274
59.599473	1999.000642	20.298291
59.554980	1987.343703	20.303309
59.726904	1987.578371	20.308327
59.483844	1996.592190	20.313344
59.964768	1996.902469	20.318362
60.046908	2020.334454	20.323379
59.765146	2020.089506	20.328397
59.882867	2011.605376	20.333415
59.984126	2025.830832	20.338432
60.336823	2012.914376	20.343450
59.816001	2016.596115	20.348467
60.185093	2030.157921	20.353485
60.631201	2013.096759	20.358503
60.340765	2022.487738	20.363520
60.661519	2018.761838	20.368538
60.482181	2019.840122	20.373555
60.257971	2027.384659	20.378573
60.295991	2027.138338	20.383591
60.048638	2036.915902	20.388608
60.427410	2038.999835	20.393626
60.420837	2043.203139	20.398643
60.661697	2037.169931	20.403661
61.011291	2055.732362	20.408679
60.702214	2064.996528	20.413696
61.298271	2060.769510	20.418714
61.545240	2068.751418	20.423731
61.509395	2065.027859	20.428749
61.667577	2064.093905	20.433767
61.423450	2047.622992	20.438784
61.637487	2038.881554	20.443802
61.081207	2035.078817	20.448819
61.449241	2048.017176	20.453837
61.748769	2060.198757	20.458855
61.525862	2069.593544	20.463872
61.805921	2067.922460	20.468890
61.585547	2066.146832	20.473907
61.715812	2065.752161	20.478925
62.159982	2065.977186	20.483943
61.867016	2067.721549	20.488960
61.822958	2055.722351	20.493978
61.950211	2059.255059	20.498995
61.720212	2063.454417	20.504013
61.875633	2064.471762	20.509031
61.868369	2074.503305	20.514048
61.948757	2081.464741	20.519066
62.115237	2085.172066	20.524083
62.168438	2089.654471	20.529101
62.531510	2093.539489	20.534119
62.372461	2087.462239	20.539136
62.123589	2089.018195	20.544154
62.074010	2106.423125	20.549171
62.168392	2111.307390	20.554189
62.543325	2119.215772	20.559207
62.239648	2112.642758	20.564224
62.936218	2134.002644	20.569242
63.133398	2133.909895	20.574259
63.286586	2136.080801	20.579277
63.412830	2138.912096	20.584295
63.491791	2141.661847	20.589312
63.566534	2129.764185	20.594330
63.486103	2117.091807	20.599347
63.517346	2096.192434	20.604365
63.448032	2094.727233	20.609383
63.429230	2104.070921	20.614400
63.701965	2103.938888	20.619418
63.890289	2101.006968	20.624435
63.733078	2100.113030	20.629453
63.776338	2092.563260	20.634471
63.485225	2104.565894	20.639488
63.489406	2102.675125	20.644506
63.921829	2119.430557	20.649523
63.911958	2120.980015	20.654541
64.179798	2118.064060	20.659559
63.729707	2123.578658	20.664576
64.087998	2118.135836	20.669594
64.164301	2125.550344	20.674611
63.870698	2112.316397	20.679629
64.514873	2107.878637	20.684647
64.327654	2127.585585	20.689664
64.184340	2120.297410	20.694682
64.085159	2127.106704	20.699699
64.169626	2147.335637	20.704717
64.614758	2146.430940	20.709735
64.792974	2156.586160	20.714752
64.684245	2153.316789	20.719770
64.742187	2155.719618	20.724787
64.619012	2154.255849	20.729805
64.758916	2154.880480	20.734823
64.623049	2159.896984	20.739840
64.863341	2174.177116	20.744858
65.185764	2171.443066	20.749875
65.163717	2181.239715	20.754893
65.357929	2180.548223	20.759911
65.222958	2174.962245	20.764928
65.598892	2181.044445	20.769946
65.765336	2177.798012	20.774963
65.419829	2171.160243	20.779981
66.030563	2171.815187	20.784999
65.733373	2174.211859	20.790016
65.567540	2174.582773	20.795034
65.552581	2179.059560	20.800051
65.601192	2185.399116	20.805069
66.186680	2198.167732	20.810087
66.096008	2208.341129	20.815104
66.425256	2201.006955	20.820122
66.270355	2199.477960	20.825139
66.216765	2204.469436	20.830157
66.385526	2196.119673	20.835175
66.569147	2199.999391	20.840192
66.515203	2205.528348	20.845210
66.617196	2192.828458	20.850227
66.365206	2198.779982	20.855245
66.560432	2192.410557	20.860263
66.804848	2203.953323	20.865280
66.753421	2196.742814	20.870298
66.951116	2185.994478	20.875315
66.871110	2200.725716	20.880333
66.908180	2190.444540	20.885351
66.808409	2206.433826	20.890368
67.135292	2201.730455	20.895386
66.861294	2195.760781	20.900403
66.956762	2198.685769	20.905421
67.411259	2204.642368	20.910439
67.223690	2225.830654	20.915456
67.317596	2220.602840	20.920474
67.630937	2213.465789	20.925491
67.341103	2216.188426	20.930509
67.711767	2213.049515	20.935527
67.624610	2214.389724	20.940544
67.717802	2218.213551	20.945562
67.617724	2208.209019	20.950579
67.615729	2206.750771	20.955597
67.877622	2214.448777	20.960615
67.771873	2218.457125	20.965632
67.387767	2238.418081	20.970650
67.860110	2242.201183	20.975667
67.963571	2241.623931	20.980685
68.514192	2244.753103	20.985703
68.214929	2249.646683	20.990720
67.935605	2243.774333	20.995738
68.352375	2242.505022	21.000755
68.195603	2243.807151	21.005773
68.475283	2258.028476	21.010791
68.521495	2264.179478	21.015808
68.756280	2268.642498	21.020826
68.890565	2260.571649	21.025843
68.702268	2273.297182	21.030861
68.766238	2264.018238	21.035879
68.869977	2268.439568	21.040896
68.815030	2273.254906	21.045914
69.260059	2257.541744	21.050931
69.171130	2266.348300	21.055949
69.197870	2262.472593	21.060967
69.150326	2287.630854	21.065984
69.235830	2298.960228	21.071002
69.340200	2295.094101	21.076019
69.150844	2299.540741	21.081037
69.511085	2289.248905	21.086055
69.330542	2297.237936	21.091072
69.338717	2299.177747	21.096090
70.015433	2305.079086	21.101107
69.797025	2326.130089	21.106125
70.002509	2312.828688	21.111143
70.114353	2316.447473	21.116160
69.998967	2313.058693	21.121178
70.409533	2306.532301	21.126195
70.302205	2313.248138	21.131213
70.252477	2302.186738	21.136231
70.338193	2317.658002	21.141248
70.585049	2307.980230	21.146266
70.586718	2305.751648	21.151283
70.371345	2308.175739	21.156301
70.644743	2301.956325	21.161319
70.858397	2310.068683	21.166336
70.376868	2314.734578	21.171354
70.745755	2315.891799	21.176371
71.064415	2326.526654	21.181389
71.117586	2332.654877	21.186407
71.041038	2330.669568	21.191424
71.055671	2337.806186	21.196442
71.555567	2331.099631	21.201459
70.979074	2338.108527	21.206477
70.960367	2327.860907	21.211495
71.095885	2333.544767	21.216512
71.529812	2357.295800	21.221530
71.660540	2352.068539	21.226547
71.611978	2356.452904	21.231565
71.776929	2354.839041	21.236583
72.027684	2354.240153	21.241600
71.985614	2361.220416	21.246618
71.991790	2356.306309	21.251635
71.864970	2362.270242	21.256653
72.309226	2359.856160	21.261671
72.159083	2353.339514	21.266688
72.002836	2359.578804	21.271706
72.316632	2352.085299	21.276723
72.565553	2349.803173	21.281741
72.265957	2348.176461	21.286759
72.554531	2356.583145	21.291776
72.176017	2356.579811	21.296794
72.588967	2364.301308	21.301811
72.575834	2375.254138	21.306829
72.450021	2380.011554	21.311847
72.887344	2381.727162	21.316864
72.861635	2376.988022	21.321882
72.857725	2378.430214	21.326899
72.591984	2385.757773	21.331917
72.878851	2385.594265	21.336935
73.070076	2382.747643	21.341952
72.981759	2398.910828	21.346970
73.541708	2391.119448	21.351987
73.526520	2405.824793	21.357005
73.657937	2401.149397	21.362023
74.061066	2392.834348	21.367040
73.638861	2396.542760	21.372058
73.787375	2400.070844	21.377075
73.841112	2395.779983	21.382093
73.841813	2395.654408	21.387111
73.758449	2388.054985	21.392128
73.431385	2406.047559	21.397146
74.029309	2391.726734	21.402163
73.887855	2400.096765	21.407181
74.162145	2406.878596	21.412199
74.312314	2415.553123	21.417216
74.038533	2420.075590	21.422234
74.579482	2425.775822	21.427251
74.588243	2428.740802	21.432269
74.324237	2421.959502	21.437287
74.392666	2416.128330	21.442304
74.304069	2425.063667	21.447322
74.707330	2427.390069	21.452339
74.938579	2443.918520	21.457357
75.137217	2447.057587	21.462375
75.285183	2447.274969	21.467392
75.219274	2447.974638	21.472410
75.319994	2437.530391	21.477427
75.186062	2439.601629	21.482445
75.345811	2442.369162	21.487463
75.641312	2435.506238	21.492480
75.170509	2445.896282	21.497498
75.116235	2437.893966	21.502515
75.411356	2439.258303	21.507533
75.750318	2460.269564	21.512551
75.842514	2464.652702	21.517568
75.705634	2464.814881	21.522586
76.242737	2466.468700	21.527603
76.094172	2477.639707	21.532621
76.193320	2470.534855	21.537639
76.352839	2465.043720	21.542656
76.019818	2467.826309	21.547674
76.115865	2470.200829	21.552691
76.379541	2464.697172	21.557709
76.335006	2464.253872	21.562727
76.859720	2467.466912	21.567744
76.581990	2464.577838	21.572762
76.611250	2459.755945	21.577779
76.539670	2476.061329	21.582797
76.773116	2480.977019	21.587815
76.677151	2488.322975	21.592832
76.703760	2489.748706	21.597850
76.768473	2485.404426	21.602867
77.164020	2488.908558	21.607885
76.783889	2497.076808	21.612903
77.163141	2503.592076	21.617920
77.578149	2509.489187	21.622938
77.368887	2519.217042	21.627955
77.543482	2514.158851	21.632973
77.222858	2516.006666	21.637991
77.736292	2503.159654	21.643008
77.728886	2524.245283	21.648026
77.870018	2512.186328	21.653043
78.358125	2500.099067	21.658061
77.960651	2510.632138	21.663079
78.073368	2497.314443	21.668096
78.130846	2501.702158	21.673114
78.043939	2507.754819	21.678131
78.321823	2511.015825	21.683149
77.816587	2531.166117	21.688167
78.403204	2538.144338	21.693184
78.207287	2538.810022	21.698202
78.429801	2537.976813	21.703219
78.769479	2534.959906	21.708237
78.403080	2534.750616	21.713255
78.804096	2541.449709	21.718272
79.206616	2562.130487	21.723290
79.352284	2557.865308	21.728307
79.115797	2543.169087	21.733325
78.763378	2544.728845	21.738343
79.351220	2553.682970	21.743360
78.961011	2557.030589	21.748378
79.299164	2560.788743	21.753395
79.309960	2558.758231	21.758413
79.373919	2559.702954	21.763431
79.528806	2554.858261	21.768448
79.519512	2565.096374	21.773466
79.682812	2573.966072	21.778483
79.648337	2586.969953	21.783501
79.539820	2589.740983	21.788519
80.052556	2593.265107	21.793536
80.013638	2588.135152	21.798554
80.008839	2586.142261	21.803571
80.081086	2586.962376	21.808589
79.791329	2610.575732	21.813607
80.118260	2611.256036	21.818624
80.372440	2616.644745	21.823642
80.502937	2620.065225	21.828659
80.670380	2615.645628	21.833677
80.495544	2617.521287	21.838695
80.616926	2621.043283	21.843712
80.802405	2633.928496	21.848730
81.030854	2637.498127	21.853747
81.422841	2633.657527	21.858765
81.451135	2636.676796	21.863783
81.281646	2635.549804	21.868800
81.466872	2631.285536	21.873818
81.538066	2626.370422	21.878835
81.605396	2621.889047	21.883853
81.389982	2631.367975	21.888871
81.614315	2624.596285	21.893888
81.788785	2628.979234	21.898906
81.761664	2633.071526	21.903923
81.873860	2618.314350	21.908941
81.997244	2627.094224	21.913959
81.988676	2624.118425	21.918976
82.106086	2641.630170	21.923994
82.245714	2646.839812	21.929011
82.421384	2645.897811	21.934029
82.227045	2662.335533	21.939047
82.509248	2658.425698	21.944064
82.782956	2654.633813	21.949082
82.331432	2654.910693	21.954099
82.696579	2653.167584	21.959117
82.590103	2660.812624	21.964135
82.810377	2656.049600	21.969152
82.692213	2655.262557	21.974170
82.943809	2668.078579	21.979187
83.129397	2669.964257	21.984205
82.931893	2680.357238	21.989223
82.904501	2677.846388	21.994240
82.975831	2675.913720	21.999258
82.765708	2680.242637	22.004275
83.451923	2687.136321	22.009293
83.277033	2712.680550	22.014311
83.461424	2710.959882	22.019328
83.695015	2710.887876	22.024346
83.492705	2706.883043	22.029363
83.901684	2706.956024	22.034381
83.404902	2708.533401	22.039399
83.697872	2717.641965	22.044416
83.845481	2726.063528	22.049434
84.015037	2727.692401	22.054451
84.135776	2727.411505	22.059469
84.235490	2733.481782	22.064487
84.404372	2730.713212	22.069504
84.690919	2736.802952	22.074522
84.611063	2753.847844	22.079539
85.072416	2750.765078	22.084557
85.209787	2756.209793	22.089575
85.362458	2756.006292	22.094592
85.274803	2734.495783	22.099610
85.199541	2729.276122	22.104627
85.342820	2719.710922	22.109645
85.371169	2720.415864	22.114663
85.699919	2730.472121	22.119680
85.364167	2722.699347	22.124698
85.125749	2740.563053	22.129715
85.739926	2743.124287	22.134733
85.673776	2752.791187	22.139751
85.928949	2752.223446	22.144768
85.927475	2753.801500	22.149786
85.482990	2753.601590	22.154803
86.023642	2753.114543	22.159821
85.640002	2748.397149	22.164839
85.989220	2758.365778	22.169856
86.365291	2766.862142	22.174874
86.103440	2767.944688	22.179891
86.245219	2768.306417	22.184909
85.903692	2776.933022	22.189927
86.357682	2782.142237	22.194944
86.519287	2795.183910	22.199962
86.549029	2789.316088	22.204979
86.842717	2796.388208	22.209997
86.908803	2796.982960	22.215015
86.814066	2790.663665	22.220032
86.707129	2793.266740	22.225050
86.684267	2820.235294	22.230067
87.094597	2819.548153	22.235085
87.171863	2819.144129	22.240103
87.532884	2832.913897	22.245120
87.648341	2824.061168	22.250138
87.394377	2824.667966	22.255155
87.768276	2837.097314	22.260173
87.793501	2845.405337	22.265191
87.817133	2848.795527	22.270208
88.249891	2847.286103	22.275226
88.121200	2850.646786	22.280243
88.422809	2845.084349	22.285261
88.336016	2847.769932	22.290279
88.425780	2838.951372	22.295296
88.533239	2837.435964	22.300314
88.270357	2839.757363	22.305331
88.763933	2842.701996	22.310349
88.484930	2847.131741	22.315367
88.755505	2846.188189	22.320384
89.178625	2856.098184	22.325402
89.225242	2860.369680	22.330419
89.132216	2855.918726	22.335437
88.848991	2856.860710	22.340455
89.230684	2858.125313	22.345472
89.201422	2861.634902	22.350490
89.145194	2864.554816	22.355507
89.582417	2853.735257	22.360525
89.524534	2853.106346	22.365543
89.386859	2854.137231	22.370560
89.510933	2863.793178	22.375578
89.276959	2873.959631	22.380595
89.596609	2886.975606	22.385613
89.541852	2890.854807	22.390631
89.258887	2898.415791	22.395648
89.870828	2900.243110	22.400666
89.882429	2921.861605	22.405683
90.261857	2909.345138	22.410701
90.452608	2918.721552	22.415719
90.553402	2912.321798	22.420736
90.717055	2908.558312	22.425754
90.375959	2920.982085	22.430771
90.858285	2927.272969	22.435789
91.014750	2938.546963	22.440807
91.094906	2950.983302	22.445824
91.332833	2939.256446	22.450842
91.203443	2938.572436	22.455859
91.088173	2937.216741	22.460877
91.464161	2934.379589	22.465895
91.493046	2930.767163	22.470912
91.597881	2934.504980	22.475930
91.404271	2938.346548	22.480947
91.875310	2944.527094	22.485965
91.829914	2946.337261	22.490983
91.945201	2958.788659	22.496000
92.340319	2967.778480	22.501018
92.012410	2961.174466	22.506035
92.174302	2960.399310	22.511053
92.731521	2961.304516	22.516071
92.444705	2955.881991	22.521088
92.833055	2960.143787	22.526106
92.773319	2954.668703	22.531123
92.944783	2957.565109	22.536141
92.760178	2957.324135	22.541159
92.754243	2967.574161	22.546176
93.041301	2951.231287	22.551194
92.768446	2960.363594	22.556211
92.914331	2951.960912	22.561229
93.317001	2968.641082	22.566247
93.150774	2974.031013	22.571264
93.311205	2986.630877	22.576282
93.481041	2987.212396	22.581299
93.617173	2980.198049	22.586317
93.574704	2981.399809	22.591335
93.485796	2983.458151	22.596352
93.804057	2979.462339	22.601370
93.722232	2995.656959	22.606387
93.628151	3002.048036	22.611405
93.840408	3007.860001	22.616423
93.751769	3018.438349	22.621440
93.935032	3013.981372	22.626458
94.118550	3038.150533	22.631475
94.252342	3037.869833	22.636493
94.786660	3029.485481	22.641511
94.354917	3047.885922	22.646528
94.435509	3037.027640	22.651546
94.466774	3054.677746	22.656563
95.094476	3068.361832	22.661581
95.332825	3056.960045	22.666599
95.460767	3058.531270	22.671616
95.301433	3049.967241	22.676634
95.191100	3051.648002	22.681651
95.216523	3054.876509	22.686669
95.310132	3053.947284	22.691687
95.321994	3055.403464	22.696704
95.644687	3047.565999	22.701722
95.417854	3061.567173	22.706739
95.482790	3083.038071	22.711757
96.051920	3084.087391	22.716775
95.908054	3088.750364	22.721792
96.241963	3080.500751	22.726810
96.001668	3079.505932	22.731827
96.118616	3090.082969	22.736845
96.797897	3094.493896	22.741863
96.643549	3100.692216	22.746880
97.115093	3098.159324	22.751898
96.859676	3099.988533	22.756915
97.061686	3102.521607	22.761933
97.359019	3099.635239	22.766951
97.114039	3100.317731	22.771968
97.210122	3098.830167	22.776986
97.358299	3098.756947	22.782003
97.893928	3095.416126	22.787021
97.802353	3096.730366	22.792039
97.166730	3103.283989	22.797056
97.526897	3092.556167	22.802074
97.836929	3089.879529	22.807091
97.465044	3101.425783	22.812109
97.554723	3092.105080	22.817127
97.665358	3120.220269	22.822144
97.736679	3114.802176	22.827162
97.643140	3133.440450	22.832179
97.788430	3137.424792	22.837197
97.951790	3144.954913	22.842215
97.760059	3150.402282	22.847232
97.763845	3159.313293	22.852250
98.218262	3171.577201	22.857267
98.452125	3187.383891	22.862285
98.928935	3178.792818	22.867303
99.002660	3179.617840	22.872320
99.043356	3199.560477	22.877338
99.427281	3204.810968	22.882355
99.504565	3209.808658	22.887373
99.948057	3196.226525	22.892391
99.973119	3199.045631	22.897408
100.130313	3196.793140	22.902426
100.064057	3176.961323	22.907443
100.054562	3172.198387	22.912461
100.114189	3163.776012	22.917479
99.826903	3173.393950	22.922496
99.983310	3174.883695	22.927514
100.520193	3184.958155	22.932531
100.468870	3186.500407	22.937549
100.476420	3189.070023	22.942567
100.629093	3201.320129	22.947584
100.299945	3197.524770	22.952602
100.456882	3192.154293	22.957619
100.560814	3191.210752	22.962637
100.871949	3206.958600	22.967655
100.772110	3216.008467	22.972672
100.932093	3217.183025	22.977690
100.951871	3220.675913	22.982707
100.737618	3222.619593	22.987725
101.318270	3229.511708	22.992743
101.395453	3243.909998	22.997760
101.416912	3254.421453	23.002778
101.634236	3249.382332	23.007795
101.507237	3247.613547	23.012813
101.499592	3252.162666	23.017831
101.403945	3253.586266	23.022848
102.008366	3261.135158	23.027866
102.380815	3269.117779	23.032883
101.936954	3276.516193	23.037901
102.342684	3268.506979	23.042919
102.087294	3280.805024	23.047936
102.041133	3281.220721	23.052954
102.669610	3292.497930	23.057971
102.564174	3303.969899	23.062989
102.739654	3306.855074	23.068007
102.907023	3311.188599	23.073024
102.950221	3300.240646	23.078042
102.801073	3303.652454	23.083059
103.009872	3321.735722	23.088077
104.079935	3322.041418	23.093095
103.698208	3324.566836	23.098112
103.672418	3326.956148	23.103130
103.797709	3329.046795	23.108147
103.921470	3326.758084	23.113165
104.115056	3323.893184	23.118183
103.830467	3320.805061	23.123200
104.060843	3323.734700	23.128218
104.230208	3321.539238	23.133235
104.174484	3327.514997	23.138253
104.323526	3339.533110	23.143271
104.283201	3347.365193	23.148288
104.348658	3350.198900	23.153306
104.399301	3354.116676	23.158323
104.499264	3363.016210	23.163341
104.687213	3369.968683	23.168359
104.982492	3383.926616	23.173376
105.197164	3380.999153	23.178394
105.081998	3384.254549	23.183411
105.075492	3387.397062	23.188429
105.400446	3401.350491	23.193447
105.688145	3408.301034	23.198464
105.302304	3415.779287	23.203482
105.476111	3412.275447	23.208499
105.316407	3419.879664	23.213517
105.824428	3427.479643	23.218535
106.303725	3431.413878	23.223552
106.526281	3423.876697	23.228570
106.877713	3421.630208	23.233587
106.674971	3424.295711	23.238605
106.590577	3419.506120	23.243623
106.889321	3415.464212	23.248640
106.840418	3415.249586	23.253658
107.157380	3409.750953	23.258675
106.893284	3423.431810	23.263693
107.295260	3415.071135	23.268711
106.980742	3410.769700	23.273728
107.322867	3415.291274	23.278746
107.520319	3432.083487	23.283763
107.332158	3443.902363	23.288781
107.242905	3438.184723	23.293799
107.672446	3443.857322	23.298816
107.782472	3450.268337	23.303834
107.836837	3448.228528	23.308851
107.749201	3455.045543	23.313869
108.119767	3468.769408	23.318887
107.797204	3477.292849	23.323904
108.067078	3476.183611	23.328922
108.407092	3469.560142	23.333939
108.357920	3489.520391	23.338957
108.588780	3495.552714	23.343975
108.856585	3500.450441	23.348992
108.843364	3507.390608	23.354010
108.802916	3509.348858	23.359027
108.799295	3503.018913	23.364045
108.747382	3496.841865	23.369063
109.032330	3520.722900	23.374080
109.254390	3527.973375	23.379098
109.475080	3530.284897	23.384115
109.383536	3532.819002	23.389133
109.504105	3529.952767	23.394151
109.704334	3538.395589	23.399168
109.911305	3544.595686	23.404186
110.139329	3547.275333	23.409203
110.027881	3557.964527	23.414221
110.493799	3549.345526	23.419239
110.624457	3549.050375	23.424256
110.549189	3547.329691	23.429274
110.709564	3539.633044	23.434291
110.177490	3546.097647	23.439309
110.490934	3554.867445	23.444327
110.725395	3574.896998	23.449344
110.911845	3573.609416	23.454362
111.272125	3568.492581	23.459379
111.123755	3575.178348	23.464397
111.474998	3577.697423	23.469415
111.337563	3585.032253	23.474432
111.629732	3595.111666	23.479450
112.074985	3601.866897	23.484467
111.922656	3602.114330	23.489485
112.017682	3604.791200	23.494503
112.226025	3596.481389	23.499520
112.227795	3597.606572	23.504538
112.550687	3599.400332	23.509555
112.345963	3606.333662	23.514573
112.404997	3593.715348	23.519591
112.589966	3606.790451	23.524608
112.311136	3631.623375	23.529626
112.383574	3622.608793	23.534643
112.729584	3632.422983	23.539661
112.683528	3630.442696	23.544679
112.939054	3652.041503	23.549696
113.077078	3653.979671	23.554714
113.111373	3646.639323	23.559731
113.022231	3659.560616	23.564749
113.485193	3671.694748	23.569767
113.962884	3670.442808	23.574784
113.562472	3685.300943	23.579802
113.789816	3684.234958	23.584819
113.804791	3684.165678	23.589837
113.761986	3705.319005	23.594855
114.316806	3711.880530	23.599872
114.236350	3718.017640	23.604890
114.889678	3710.844491	23.609907
114.564847	3710.987005	23.614925
114.774905	3705.504000	23.619943
114.830644	3731.358997	23.624960
115.127489	3741.057758	23.629978
115.335288	3739.316567	23.634995
115.079273	3734.676964	23.640013
115.369419	3737.946046	23.645031
115.674935	3734.508529	23.650048
115.377459	3734.017294	23.655066
115.472956	3729.286813	23.660083
115.826110	3744.229322	23.665101
115.914832	3751.359045	23.670119
116.299704	3752.683444	23.675136
115.769979	3758.431112	23.680154
116.354509	3752.193477	23.685171
116.687863	3748.351688	23.690189
116.606425	3740.351232	23.695207
116.663293	3737.073402	23.700224
116.787902	3738.935052	23.705242
116.951332	3726.301315	23.710259
116.771497	3740.476833	23.715277
117.261211	3756.415386	23.720295
117.530867	3756.297245	23.725312
117.402323	3769.286971	23.730330
117.449474	3763.513946	23.735347
117.634185	3771.568466	23.740365
117.327268	3765.605997	23.745383
117.622536	3762.076851	23.750400
117.206008	3763.076787	23.755418
117.296463	3774.915540	23.760435
117.758796	3785.151573	23.765453
117.915919	3779.523350	23.770471
118.678870	3782.610996	23.775488
118.251776	3810.457746	23.780506
118.519259	3805.344386	23.785523
118.864571	3818.466751	23.790541
118.962650	3819.074360	23.795559
118.978781	3813.747853	23.800576
118.570886	3813.140626	23.805594
118.979991	3809.963146	23.810611
119.163285	3833.558692	23.815629
119.166243	3844.682747	23.820647
119.267751	3849.662851	23.825664
119.351451	3844.953976	23.830682
119.456501	3849.031002	23.835699
119.676603	3870.428859	23.840717
119.329060	3873.720467	23.845735
119.810370	3878.169913	23.850752
119.764740	3882.555795	23.855770
120.218150	3896.436424	23.860787
120.270118	3890.382200	23.865805
120.167306	3904.876657	23.870823
120.914489	3914.654138	23.875840
121.119435	3924.580070	23.880858
121.315803	3924.545333	23.885875
121.323072	3921.165031	23.890893
121.473514	3927.260056	23.895911
122.022282	3925.810869	23.900928
121.770467	3923.082213	23.905946
121.555513	3912.654989	23.910963
121.832900	3916.458583	23.915981
121.910249	3919.779473	23.920999
122.123222	3905.429265	23.926016
121.917317	3911.264733	23.931034
121.926509	3912.306021	23.936051
122.351059	3929.106845	23.941069
122.334035	3942.763784	23.946087
122.451975	3930.502430	23.951104
122.540581	3932.711059	23.956122
122.938608	3932.940616	23.961139
122.951551	3943.923698	23.966157
122.762042	3963.180118	23.971175
123.085890	3968.020282	23.976192
122.895211	3976.933636	23.981210
123.030935	3970.570981	23.986227
123.350137	3983.089449	23.991245
123.452319	3988.645950	23.996263
123.748286	3993.322209	24.001280
123.556570	3991.686906	24.006298
124.078658	3988.260729	24.011315
124.021501	3999.906736	24.016333
124.350991	4016.611565	24.021351
124.811066	4022.644338	24.026368
124.882942	4020.229846	24.031386
124.874902	4018.360949	24.036403
124.988904	4015.577223	24.041421
124.703580	4014.504743	24.046439
124.879688	4013.284991	24.051456
125.070845	4018.919699	24.056474
125.273876	4017.405680	24.061491
125.133332	4002.010990	24.066509
124.902000	4025.639641	24.071527
125.487500	4022.444728	24.076544
125.778393	4035.452251	24.081562
125.757061	4039.054900	24.086579
125.597339	4035.816411	24.091597
125.607930	4054.190076	24.096615
126.378947	4044.153152	24.101632
126.091055	4061.637516	24.106650
126.536535	4057.904273	24.111667
126.587152	4053.578825	24.116685
126.450174	4058.929240	24.121703
126.973837	4067.161295	24.126720
127.050818	4085.393275	24.131738
127.063555	4081.383588	24.136755
127.227546	4080.030382	24.141773
127.243007	4088.474168	24.146791
127.717259	4081.330897	24.151808
127.582481	4098.333187	24.156826
127.605451	4110.706284	24.161843
127.745414	4120.887233	24.166861
127.704941	4120.964161	24.171879
128.004025	4116.464466	24.176896
128.032959	4131.918973	24.181914
128.363426	4147.155041	24.186931
128.157728	4143.098812	24.191949
128.162144	4149.781972	24.196967
128.575635	4167.738614	24.201984
128.707499	4175.841862	24.207002
128.558236	4180.988019	24.212019
128.358190	4190.689787	24.217037
128.809564	4199.400099	24.222055
129.454787	4201.722157	24.227072
129.129291	4211.120244	24.232090
129.309598	4214.706875	24.237107
129.891202	4221.584315	24.242125
129.759707	4233.929531	24.247143
130.334500	4232.631941	24.252160
130.395842	4235.657073	24.257178
130.551766	4231.863839	24.262195
130.689933	4230.738555	24.267213
130.684937	4244.028350	24.272231
131.330661	4244.965848	24.277248
130.876771	4255.964224	24.282266
130.972349	4254.313617	24.287283
131.026524	4246.832666	24.292301
131.338855	4250.651820	24.297319
131.439876	4246.493593	24.302336
131.463356	4244.702930	24.307354
131.102557	4255.604777	24.312371
131.347066	4272.255434	24.317389
131.474984	4285.066488	24.322407
131.868033	4294.781955	24.327424
132.125491	4309.673515	24.332442
132.042087	4313.886606	24.337459
132.386254	4308.060269	24.342477
132.241140	4306.595988	24.347495
132.609275	4318.346651	24.352512
132.771648	4332.209701	24.357530
132.704313	4329.296072	24.362547
132.973247	4327.758513	24.367565
132.979326	4336.386694	24.372583
133.414657	4335.620936	24.377600
133.609159	4341.624562	24.382618
133.480660	4350.062396	24.387635
133.670145	4343.257544	24.392653
133.375795	4352.012653	24.397671
133.807162	4350.556091	24.402688
133.953407	4356.649617	24.407706
133.981910	4378.818209	24.412723
134.589587	4374.916282	24.417741
134.292226	4374.837282	24.422759
134.273230	4367.882652	24.427776
134.605451	4384.307845	24.432794
134.218123	4404.780442	24.437811
134.594671	4401.559409	24.442829
134.782603	4411.140375	24.447847
134.922541	4422.007473	24.452864
135.017637	4434.803607	24.457882
134.662195	4437.258298	24.462899
135.114962	4445.478666	24.467917
135.333247	4460.734400	24.472935
135.989476	4469.380233	24.477952
136.239320	4481.148241	24.482970
136.476775	4496.381935	24.487987
136.690863	4486.427490	24.493005
136.659937	4483.516467	24.498023
136.692978	4484.141170	24.503040
136.819867	4488.631360	24.508058
136.645869	4488.510671	24.513075
136.918801	4501.972820	24.518093
137.151691	4515.194320	24.523111
137.148892	4515.907650	24.528128
137.296569	4516.008558	24.533146
137.408218	4541.994242	24.538163
137.590588	4547.889700	24.543181
137.672924	4545.899459	24.548199
137.538796	4546.598307	24.553216
137.954767	4565.934780	24.558234
137.837530	4578.352722	24.563251
138.132632	4574.811218	24.568269
138.396849	4600.205491	24.573287
138.822946	4600.695819	24.578304
139.169785	4592.116445	24.583322
139.245784	4605.786911	24.588339
139.545730	4593.313771	24.593357
139.551447	4602.172910	24.598375
139.627637	4593.869097	24.603392
139.731196	4595.121621	24.608410
139.651422	4623.169438	24.613427
140.251586	4612.504414	24.618445
139.788752	4624.899280	24.623463
139.667710	4628.090930	24.628480
140.250129	4625.178354	24.633498
139.984957	4647.110064	24.638515
140.490951	4654.115198	24.643533
140.839880	4658.319808	24.648551
140.562708	4657.611358	24.653568
140.995765	4671.163700	24.658586
141.050208	4680.820484	24.663603
141.833260	4681.360401	24.668621
141.483134	4682.116279	24.673639
141.290884	4680.621176	24.678656
141.524882	4682.925549	24.683674
141.640127	4690.074148	24.688691
141.279510	4697.478735	24.693709
141.634154	4712.798770	24.698727
142.017145	4711.960543	24.703744
142.457457	4726.645026	24.708762
142.363167	4745.749603	24.713779
142.621394	4738.452789	24.718797
142.543220	4737.603493	24.723815
142.741841	4742.804858	24.728832
142.950256	4748.792161	24.733850
142.948204	4768.466650	24.738867
143.376890	4765.051049	24.743885
143.618321	4771.085661	24.748903
143.735514	4771.776775	24.753920
143.619071	4753.327139	24.758938
143.672728	4777.253109	24.763955
144.151360	4779.169681	24.768973
144.409355	4783.072781	24.773991
144.089852	4786.855701	24.779008
144.251866	4785.334226	24.784026
144.482544	4803.198217	24.789043
144.473336	4805.968156	24.794061
144.447060	4822.160977	24.799079
144.730400	4819.235665	24.804096
144.918764	4831.689055	24.809114
144.703787	4839.746899	24.814131
145.130019	4856.322412	24.819149
145.363375	4873.320506	24.824167
145.755288	4873.328214	24.829184
145.910922	4865.529323	24.834202
145.486131	4879.897238	24.839219
145.904494	4884.478684	24.844237
146.281586	4899.609320	24.849255
146.094534	4908.726578	24.854272
146.923987	4919.048278	24.859290
146.861024	4929.912305	24.864307
146.902498	4931.157020	24.869325
147.318268	4927.871897	24.874343
147.042524	4924.665033	24.879360
147.523516	4925.253395	24.884378
147.689877	4942.665103	24.889395
147.369687	4947.798066	24.894413
147.540964	4946.916911	24.899431
147.827940	4949.014873	24.904448
147.763235	4960.285594	24.909466
148.106757	4972.386567	24.914483
148.423090	4975.612986	24.919501
148.275943	4987.414021	24.924519
148.350873	5008.132196	24.929536
148.671215	5007.837513	24.934554
148.455966	5019.807362	24.939571
148.862764	5032.993419	24.944589
148.881649	5037.528424	24.949607
148.975177	5058.135688	24.954624
149.370834	5060.137703	24.959642
149.524483	5072.892372	24.964659
149.861276	5078.611249	24.969677
150.301281	5082.948960	24.974695
150.576282	5091.875628	24.979712
150.779079	5080.398721	24.984730
150.762103	5088.558586	24.989747
150.785808	5081.806065	24.994765
150.776864	5081.305211	24.999783
150.863376	5090.856128	25.004800
151.303971	5100.523272	25.009818
151.228870	5105.217983	25.014835
151.061450	5105.632539	25.019853
151.585115	5105.847620	25.024871
151.970501	5133.148319	25.029888
152.193455	5146.308202	25.034906
152.158765	5145.427269	25.039923
152.317181	5143.469250	25.044941
152.444646	5144.553257	25.049959
152.504853	5146.120946	25.054976
152.686862	5136.642375	25.059994
152.626990	5145.211823	25.065011
152.872037	5160.778839	25.070029
153.051864	5167.204992	25.075047
152.953457	5163.356769	25.080064
153.125138	5167.294733	25.085082
153.420010	5187.423850	25.090099
153.403562	5192.074223	25.095117
153.370681	5205.036299	25.100135
153.658423	5215.558144	25.105152
153.966684	5213.329582	25.110170
154.073456	5227.110481	25.115187
154.151105	5226.810295	25.120205
154.307824	5235.240761	25.125223
154.525623	5252.069360	25.130240
154.679601	5246.950702	25.135258
154.682683	5263.152504	25.140275
155.022933	5266.519151	25.145293
155.209650	5273.832602	25.150311
155.078481	5290.438637	25.155328
155.628042	5287.476253	25.160346
155.228753	5305.906636	25.165363
155.572385	5307.021811	25.170381
155.992592	5304.381698	25.175399
155.886941	5323.946443	25.180416
156.373951	5324.226667	25.185434
156.449395	5332.053172	25.190451
157.014194	5344.921926	25.195469
157.173132	5353.023663	25.200487
157.265218	5359.238383	25.205504
157.661912	5347.896937	25.210522
157.520982	5352.179685	25.215539
157.520840	5358.116690	25.220557
157.943687	5347.975925	25.225575
158.044875	5359.855839	25.230592
158.122595	5383.851204	25.235610
158.119288	5384.855279	25.240627
158.496588	5369.731870	25.245645
158.607733	5372.426852	25.250663
158.663228	5382.413893	25.255680
158.899279	5391.211715	25.260698
158.850945	5398.563351	25.265715
158.766163	5409.788099	25.270733
158.917157	5404.891985	25.275751
159.216863	5433.979471	25.280768
159.411790	5428.860276	25.285786
159.344515	5440.509022	25.290803
159.448225	5467.547410	25.295821
160.063313	5459.414617	25.300839
160.057506	5468.990499	25.305856
160.596445	5481.031159	25.310874
160.536223	5492.839446	25.315891
160.733744	5502.608513	25.320909
161.216209	5486.672897	25.325927
161.161551	5483.829413	25.330944
161.211286	5510.201054	25.335962
161.693571	5519.896210	25.340979
161.776264	5518.179084	25.345997
162.151103	5517.799763	25.351015
161.636238	5520.269196	25.356032
162.036397	5518.047431	25.361050
162.115227	5518.833929	25.366067
162.021838	5538.792283	25.371085
162.308913	5545.243366	25.376103
162.060049	5553.419021	25.381120
162.538906	5562.252350	25.386138
162.932202	5572.983788	25.391155
162.979556	5579.518677	25.396173
163.453261	5593.769991	25.401191
163.067123	5605.484250	25.406208
163.366393	5604.943378	25.411226
163.429419	5607.987399	25.416243
163.637973	5625.287338	25.421261
164.391640	5627.770453	25.426279
164.040200	5635.388971	25.431296
164.338729	5639.004401	25.436314
164.422923	5640.595735	25.441331
164.672146	5646.673501	25.446349
165.041169	5651.131026	25.451367
164.878376	5650.572925	25.456384
164.683387	5652.868916	25.461402
165.384357	5673.163766	25.466419
165.427888	5682.782017	25.471437
165.779204	5678.026715	25.476455
165.672203	5681.447021	25.481472
165.507520	5701.933265	25.486490
166.078521	5702.102718	25.491507
165.934293	5716.795116	25.496525
166.568420	5730.884528	25.501543
166.648669	5743.558954	25.506560
166.479999	5731.012856	25.511578
166.977318	5741.395605	25.516595
167.323369	5761.847779	25.521613
167.256508	5760.107343	25.526631
167.220817	5774.613278	25.531648
167.827291	5785.475754	25.536666
167.880472	5794.030776	25.541683
167.906495	5795.728632	25.546701
168.174649	5802.156962	25.551719
168.401367	5816.186305	25.556736
168.305399	5820.908311	25.561754
168.899216	5821.131485	25.566771
168.498622	5845.160270	25.571789
168.934145	5845.360031	25.576807
169.440012	5854.285930	25.581824
169.421746	5855.468937	25.586842
169.447324	5864.061646	25.591859
169.665669	5877.223692	25.596877
169.859108	5880.436778	25.601895
169.533836	5893.206027	25.606912
170.116421	5899.608333	25.611930
170.724250	5898.706049	25.616947
170.449360	5910.093368	25.621965
170.639773	5919.169194	25.626983
170.860300	5929.187542	25.632000
171.209721	5927.959432	25.637018
171.282991	5944.673291	25.642035
171.118256	5953.108527	25.647053
171.472802	5967.560272	25.652071
171.839665	5970.688745	25.657088
172.282250	5982.209373	25.662106
172.360679	5980.581118	25.667123
172.408408	5988.785869	25.672141
172.648648	5985.048357	25.677159
173.001911	5981.991540	25.682176
172.833932	5980.189058	25.687194
173.118520	5998.890598	25.692212
173.477137	6014.835829	25.697229
173.539101	6012.477808	25.702247
173.528193	6011.601553	25.707264
173.590982	6015.329348	25.712282
173.946036	6035.558278	25.717300
173.982479	6045.393731	25.722317
174.161469	6043.234503	25.727335
174.297998	6049.749310	25.732352
174.366669	6072.157008	25.737370
174.511608	6066.885996	25.742388
174.599899	6080.780180	25.747405
174.902133	6075.620959	25.752423
175.100905	6091.336753	25.757440
175.114645	6091.870988	25.762458
175.437974	6090.954360	25.767476
175.321908	6110.172883	25.772493
175.340113	6120.050783	25.777511
175.708665	6128.606546	25.782528
175.951964	6144.164584	25.787546
176.573905	6143.921560	25.792564
176.512122	6149.951768	25.797581
176.531669	6157.157833	25.802599
176.903063	6177.041621	25.807616
176.992735	6177.521545	25.812634
177.416385	6189.523552	25.817652
177.544974	6200.735589	25.822669
177.686120	6209.987504	25.827687
178.032416	6209.847610	25.832704
177.514055	6201.112094	25.837722
178.254780	6213.091557	25.842740
178.208409	6234.048021	25.847757
178.401516	6234.588798	25.852775
178.614666	6246.230305	25.857792
178.745866	6262.260695	25.862810
179.024708	6261.613705	25.867828
179.023205	6279.023174	25.872845
179.277819	6297.859989	25.877863
179.433496	6297.537415	25.882880
179.760814	6318.024130	25.887898
179.821417	6319.964423	25.892916
179.821956	6332.206716	25.897933
180.291527	6342.427478	25.902951
180.622620	6352.410463	25.907968
180.411675	6355.247941	25.912986
180.915521	6363.144234	25.918004
180.871872	6388.427741	25.923021
181.224538	6380.560043	25.928039
181.469600	6385.485680	25.933056
181.534786	6408.871892	25.938074
181.709494	6411.778645	25.943092
181.809733	6416.665256	25.948109
182.040086	6427.610138	25.953127
182.124856	6435.838919	25.958144
182.109303	6452.686164	25.963162
182.607460	6457.565198	25.968180
182.829930	6465.142658	25.973197
183.047124	6479.757813	25.978215
183.319971	6484.216534	25.983232
183.567838	6504.196010	25.988250
183.624440	6499.599527	25.993268
184.017352	6506.842396	25.998285
184.385502	6526.404226	26.003303
184.614236	6523.856266	26.008320
184.542151	6536.879482	26.013338
184.682782	6524.431989	26.018356
184.490264	6523.425092	26.023373
184.958024	6537.846015	26.028391
185.352923	6541.764699	26.033408
185.083385	6540.222348	26.038426
185.496065	6548.941167	26.043444
185.664070	6575.406061	26.048461
185.838036	6577.368577	26.053479
185.947494	6575.629579	26.058496
185.852924	6605.812378	26.063514
186.190156	6601.886170	26.068532
186.235368	6614.549767	26.073549
186.684709	6629.610246	26.078567
186.817446	6631.838731	26.083584
186.588415	6637.662880	26.088602
186.766331	6657.567488	26.093620
187.146686	6670.767962	26.098637
187.501428	6684.179053	26.103655
188.004471	6702.575095	26.108672
187.995433	6711.463852	26.113690
188.120661	6699.869440	26.118708
188.242364	6705.418156	26.123725
188.166254	6715.763368	26.128743
188.865576	6717.973683	26.133760
188.567820	6736.529116	26.138778
189.003333	6755.803610	26.143796
189.286056	6757.276336	26.148813
189.437527	6770.519511	26.153831
189.908073	6771.968234	26.158848
189.857584	6788.473474	26.163866
190.324046	6779.682508	26.168884
189.780209	6795.292730	26.173901
190.268965	6813.493564	26.178919
190.523981	6818.190842	26.183936
190.488012	6834.548797	26.188954
191.152016	6833.500903	26.193972
191.215325	6845.384265	26.198989
191.283324	6867.388339	26.204007
191.757373	6871.672082	26.209024
191.403423	6884.284613	26.214042
191.829362	6892.875401	26.219060
191.993925	6906.861654	26.224077
192.289446	6916.226267	26.229095
192.530868	6924.299404	26.234112
193.106949	6937.010852	26.239130
192.681217	6936.196130	26.244148
193.081160	6949.567669	26.249165
193.372396	6961.440166	26.254183
193.880466	6954.861079	26.259200
193.688657	6992.322226	26.264218
193.924440	6991.555522	26.269236
194.279895	6996.092083	26.274253
194.442572	7006.080522	26.279271
194.425079	7008.639547	26.284288
194.568314	7030.381700	26.289306
194.947719	7021.441965	26.294324
195.409384	7038.443193	26.299341
195.228690	7046.460245	26.304359
195.226389	7041.155000	26.309376
195.476238	7069.165185	26.314394
195.615041	7070.984713	26.319412
196.166762	7090.155308	26.324429
196.375320	7104.802401	26.329447
196.408629	7100.254498	26.334464
196.026555	7110.959387	26.339482
196.584667	7119.013278	26.344500
196.935737	7137.858756	26.349517
196.736384	7157.237264	26.354535
197.506213	7156.673584	26.359552
197.556846	7176.761390	26.364570
197.729435	7189.602853	26.369588
198.139809	7188.144799	26.374605
198.637237	7219.405190	26.379623
198.683174	7221.883645	26.384640
198.566760	7229.325380	26.389658
199.089756	7218.816332	26.394676
199.385991	7236.372118	26.399693
199.132878	7261.431754	26.404711
199.504764	7247.470082	26.409728
199.663367	7261.088211	26.414746
199.802269	7275.524078	26.419764
200.291667	7277.007538	26.424781
200.396073	7286.763981	26.429799
200.471712	7285.236091	26.434816
200.416287	7292.785911	26.439834
200.424291	7303.609883	26.444852
200.639664	7309.533996	26.449869
200.751410	7327.473308	26.454887
201.163173	7333.014398	26.459904
201.134083	7356.810669	26.464922
201.210726	7361.896825	26.469940
201.816041	7366.730836	26.474957
202.050575	7393.555506	26.479975
202.465909	7401.188134	26.484992
202.328660	7402.707604	26.490010
202.808348	7422.582119	26.495028
203.202804	7421.653646	26.500045
203.318253	7433.505185	26.505063
203.370405	7439.489451	26.510080
203.561170	7460.212927	26.515098
203.568223	7471.201798	26.520116
203.894152	7476.479880	26.525133
203.732566	7482.170289	26.530151
204.319665	7503.930194	26.535168
204.312136	7518.826907	26.540186
204.648582	7525.081583	26.545204
205.179640	7529.026813	26.550221
204.829719	7546.179482	26.555239
205.525157	7553.263263	26.560256
205.604174	7569.591121	26.565274
205.818504	7577.425678	26.570292
206.203813	7587.017648	26.575309
206.209969	7601.438765	26.580327
206.730662	7598.124708	26.585344
206.874131	7606.289240	26.590362
207.000552	7617.154475	26.595380
207.464144	7618.206642	26.600397
207.309461	7629.386239	26.605415
207.849355	7639.737201	26.610432
207.944170	7660.205064	26.615450
207.925571	7663.002264	26.620468
208.111419	7660.237517	26.625485
208.298555	7681.365186	26.630503
208.667954	7688.748766	26.635520
208.695285	7696.611187	26.640538
208.620251	7719.193086	26.645556
209.395482	7719.620221	26.650573
209.305699	7739.184525	26.655591
209.651077	7749.627626	26.660608
209.608273	7757.513504	26.665626
209.795847	7772.555389	26.670644
210.016272	7782.170835	26.675661
210.108519	7795.843731	26.680679
210.655169	7806.980607	26.685696
210.851668	7816.956080	26.690714
210.999870	7828.483469	26.695732
211.241596	7840.285262	26.700749
210.980154	7856.561859	26.705767
211.622963	7867.493808	26.710784
212.181921	7878.971352	26.715802
212.057077	7899.331734	26.720820
212.576988	7898.187114	26.725837
212.803759	7908.404188	26.730855
213.403265	7921.305542	26.735872
213.468060	7933.822795	26.740890
213.215087	7943.643529	26.745908
213.237154	7934.277997	26.750925
213.538295	7945.555654	26.755943
213.576648	7958.095420	26.760960
213.987117	7961.339174	26.765978
213.762879	7973.245773	26.770996
214.002563	7986.871582	26.776013
213.914778	8005.956948	26.781031
214.459903	8012.561680	26.786048
214.449803	8033.429434	26.791066
214.908118	8050.166840	26.796084
215.402240	8059.555969	26.801101
215.502578	8074.055661	26.806119
216.012479	8082.511890	26.811136
216.113679	8101.289593	26.816154
216.218918	8105.335395	26.821172
216.347478	8115.202568	26.826189
216.841655	8135.841247	26.831207
217.129608	8140.948600	26.836224
217.324402	8142.193396	26.841242
217.694310	8158.569019	26.846260
218.305952	8161.085523	26.851277
218.277460	8169.936564	26.856295
218.199227	8168.165448	26.861312
218.218418	8167.624389	26.866330
218.612010	8181.937781	26.871348
218.837469	8188.571874	26.876365
218.968650	8213.136921	26.881383
219.549337	8223.796606	26.886400
219.397746	8225.487889	26.891418
219.414773	8245.615689	26.896436
219.669609	8251.291789	26.901453
219.695539	8268.459421	26.906471
219.852008	8285.659816	26.911488
220.116022	8302.158672	26.916506
220.184670	8325.753514	26.921524
220.763928	8340.817747	26.926541
220.818191	8347.920591	26.931559
221.278983	8363.963134	26.936576
221.567807	8377.973436	26.941594
221.598021	8392.638635	26.946612
222.108683	8408.424829	26.951629
222.330222	8419.089745	26.956647
222.560617	8429.579112	26.961664
223.111831	8436.415398	26.966682
223.049746	8443.995223	26.971700
223.482029	8443.576405	26.976717
223.519678	8469.472072	26.981735
223.715493	8470.776593	26.986752
224.112213	8479.733870	26.991770
223.925706	8493.481081	26.996788
223.912333	8503.991944	27.001805
224.379094	8518.503067	27.006823
224.605949	8531.966827	27.011840
224.925980	8540.660334	27.016858
225.047207	8552.395951	27.021876
225.283767	8566.473364	27.026893
225.264069	8588.481727	27.031911
225.654445	8593.176822	27.036928
226.083930	8612.961881	27.041946
226.164850	8628.177416	27.046964
226.525250	8635.538508	27.051981
226.769536	8651.153984	27.056999
227.184466	8662.524385	27.062016
227.554497	8678.268744	27.067034
227.584101	8680.937616	27.072052
227.890936	8690.169850	27.077069
228.007271	8704.216871	27.082087
228.043390	8701.959626	27.087104
228.256881	8725.310509	27.092122
228.219585	8733.618192	27.097140
228.822582	8737.806266	27.102157
229.089224	8762.311921	27.107175
229.219428	8767.789841	27.112192
229.536950	8779.182753	27.117210
229.588218	8799.281948	27.122228
229.968752	8804.387582	27.127245
230.100427	8807.957318	27.132263
230.450252	8827.842484	27.137280
231.351925	8838.989065	27.142298
231.051275	8835.812302	27.147316
230.985682	8826.366227	27.152333
231.500031	8847.939139	27.157351
231.513782	8863.459852	27.162368
231.859400	8863.878585	27.167386
231.995661	8886.668997	27.172404
232.149884	8887.028821	27.177421
232.155076	8900.680049	27.182439
232.093065	8910.537509	27.187456
232.616303	8925.346882	27.192474
232.753021	8954.944399	27.197492
232.952969	8965.160289	27.202509
233.441846	8973.642533	27.207527
233.172194	8995.607754	27.212544
234.057273	9009.103966	27.217562
233.839663	9034.700908	27.222580
234.168047	9044.965700	27.227597
234.805404	9062.380376	27.232615
235.064084	9082.052493	27.237632
235.619918	9083.228934	27.242650
235.164793	9100.778021	27.247668
236.034098	9099.578637	27.252685
235.865184	9124.145131	27.257703
236.074329	9131.121061	27.262720
236.649860	9143.462545	27.267738
236.844534	9155.614208	27.272756
237.329050	9154.127958	27.277773
237.145213	9172.104880	27.282791
237.283608	9189.275365	27.287808
237.879552	9200.529531	27.292826
237.711321	9219.271220	27.297844
237.978476	9223.079377	27.302861
238.385298	9247.416043	27.307879
238.323987	9257.963696	27.312896
238.987019	9269.369089	27.317914
239.121391	9288.328611	27.322932
239.375894	9297.907032	27.327949
239.595766	9318.473697	27.332967
239.701281	9322.601692	27.337984
240.202457	9341.996863	27.343002
240.251069	9348.896262	27.348020
240.679786	9365.597411	27.353037
240.802169	9372.888743	27.358055
240.711449	9380.925153	27.363072
241.012894	9404.264830	27.368090
241.068946	9409.465338	27.373108
241.257893	9439.077161	27.378125
241.734271	9452.654799	27.383143
242.007871	9475.108196	27.388160
242.441287	9478.791994	27.393178
242.785171	9497.509105	27.398196
243.027986	9504.860917	27.403213
243.096571	9520.429910	27.408231
243.308314	9549.970414	27.413248
243.558195	9555.074284	27.418266
243.836457	9570.946582	27.423284
243.984691	9582.312157	27.428301
244.404324	9601.941726	27.433319
244.765206	9609.270890	27.438336
245.114644	9627.876942	27.443354
244.709138	9632.593014	27.448372
245.213144	9642.779487	27.453389
245.655307	9661.144917	27.458407
245.696283	9675.947374	27.463424
245.920391	9673.834554	27.468442
246.259397	9697.240917	27.473460
246.499482	9698.364898	27.478477
246.642318	9709.617226	27.483495
247.070081	9735.926192	27.488512
247.546221	9741.752113	27.493530
247.392774	9757.226526	27.498548
247.922593	9754.641614	27.503565
248.165166	9761.573683	27.508583
248.311385	9780.786288	27.513600
248.663965	9783.792632	27.518618
248.536635	9803.892713	27.523636
248.864450	9810.278135	27.528653
249.288598	9827.713185	27.533671
249.327678	9840.282666	27.538688
249.735118	9855.271209	27.543706
249.845471	9872.661351	27.548724
250.125427	9887.261366	27.553741
250.875410	9890.336663	27.558759
250.584193	9911.586640	27.563776
251.171499	9921.323054	27.568794
251.204478	9933.722662	27.573812
250.954035	9958.933389	27.578829
251.494737	9968.916255	27.583847
251.758219	9999.384947	27.588864
251.872532	10003.279255	27.593882
252.030541	10028.406721	27.598900
252.382732	10045.259903	27.603917
253.119257	10057.892150	27.608935
252.961896	10081.364696	27.613952
253.536323	10090.362004	27.618970
253.841757	10127.002100	27.623988
253.818018	10128.005128	27.629005
253.925139	10139.448808	27.634023
254.206784	10168.253290	27.639040
254.648512	10186.677694	27.644058
255.292552	10191.854392	27.649076
254.928660	10213.743119	27.654093
255.652352	10228.604030	27.659111
255.921488	10246.208580	27.664128
256.173254	10257.898626	27.669146
256.118985	10275.001322	27.674164
256.632877	10284.941554	27.679181
257.192529	10307.569357	27.684199
256.916573	10316.371155	27.689216
257.670866	10334.026272	27.694234
257.855373	10335.132713	27.699252
257.919056	10358.618705	27.704269
258.464198	10370.845632	27.709287
258.547111	10377.642891	27.714304
258.527135	10393.208480	27.719322
258.852108	10415.738988	27.724340
258.846252	10428.420360	27.729357
259.496375	10440.682748	27.734375
259.476872	10462.871696	27.739392
260.022559	10474.280834	27.744410
260.038643	10497.123361	27.749428
260.248056	10510.283626	27.754445
260.464098	10526.644601	27.759463
260.669599	10543.818818	27.764480
260.903256	10566.043210	27.769498
261.510706	10577.549344	27.774516
261.423173	10596.379331	27.779533
262.131516	10606.932822	27.784551
262.224341	10622.171912	27.789568
262.699053	10641.398923	27.794586
263.195443	10658.419538	27.799604
263.147936	10662.083166	27.804621
263.522019	10659.207179	27.809639
263.387538	10683.104613	27.814656
263.906954	10689.019049	27.819674
264.171873	10703.459209	27.824692
264.057180	10713.970956	27.829709
264.733820	10731.406161	27.834727
264.941503	10751.025737	27.839744
265.109314	10759.250090	27.844762
265.643545	10780.703349	27.849780
265.715051	10784.682931	27.854797
265.736229	10798.853108	27.859815
266.059893	10808.547041	27.864832
266.123811	10834.077389	27.869850
266.661737	10850.576073	27.874868
266.524808	10875.627624	27.879885
267.031321	10886.105985	27.884903
267.147296	10911.115728	27.889920
267.426411	10925.917730	27.894938
267.833914	10947.901149	27.899956
268.045381	10968.336590	27.904973
268.371859	10982.071912	27.909991
268.813635	11000.004825	27.915008
268.884402	11018.988733	27.920026
269.313485	11041.154644	27.925044
269.088570	11061.796375	27.930061
269.933174	11076.911452	27.935079
269.945105	11112.433170	27.940096
270.237596	11120.221073	27.945114
270.620556	11136.792975	27.950132
271.040736	11164.316495	27.955149
271.020099	11171.946680	27.960167
271.460371	11198.551422	27.965184
272.081874	11207.016055	27.970202
271.999937	11221.348640	27.975220
272.362571	11242.074555	27.980237
272.540841	11249.942883	27.985255
272.596200	11278.551229	27.990272
273.015097	11292.547277	27.995290
273.347100	11313.885023	28.000308
273.791448	11338.633070	28.005325
274.346610	11355.228693	28.010343
274.267539	11369.526268	28.015360
274.713857	11393.208852	28.020378
274.791905	11393.665650	28.025396
275.104998	11406.956031	28.030413
275.870748	11422.541461	28.035431
275.902695	11440.186577	28.040448
275.964905	11458.416044	28.045466
276.530126	11462.654438	28.050484
276.346969	11484.644964	28.055501
277.069971	11506.600558	28.060519
277.208223	11516.060877	28.065536
277.616455	11532.988282	28.070554
278.113459	11542.127653	28.075572
278.209452	11548.750691	28.080589
278.353862	11564.524201	28.085607
278.926150	11573.865436	28.090624
278.878484	11598.509381	28.095642
279.119914	11597.029280	28.100660
279.268271	11623.419885	28.105677
279.621769	11637.904524	28.110695
279.791810	11654.581537	28.115712
280.113056	11667.344467	28.120730
280.844164	11686.936843	28.125748
280.284773	11709.071892	28.130765
281.023568	11712.550448	28.135783
281.494858	11731.141127	28.140800
281.186177	11738.077053	28.145818
281.877521	11759.195175	28.150836
281.642112	11777.679121	28.155853
282.147358	11789.510327	28.160871
282.118905	11814.247543	28.165888
282.218187	11835.202182	28.170906
282.579472	11853.856909	28.175924
282.760855	11892.615805	28.180941
283.205853	11903.650248	28.185959
283.787949	11925.128624	28.190976
283.823484	11948.990326	28.195994
283.923984	11968.421112	28.201012
284.595942	11993.075756	28.206029
284.673278	12012.652253	28.211047
285.091717	12036.167053	28.216064
285.472978	12063.347134	28.221082
285.976960	12076.951578	28.226100
286.220017	12100.153544	28.231117
286.378766	12116.555554	28.236135
286.759363	12134.692108	28.241152
286.605462	12163.092396	28.246170
287.082458	12170.987366	28.251188
287.334754	12198.866636	28.256205
287.664690	12225.776560	28.261223
288.117318	12245.700940	28.266240
287.970629	12274.502071	28.271258
288.689858	12290.920218	28.276276
289.154702	12315.641154	28.281293
289.433865	12326.917653	28.286311
290.170594	12351.943482	28.291328
290.311553	12360.672646	28.296346
290.533264	12377.285118	28.301364
290.724276	12398.116565	28.306381
291.270250	12415.792695	28.311399
291.415923	12428.393031	28.316416
291.807199	12446.167291	28.321434
292.327459	12440.565753	28.326452
292.364974	12475.315617	28.331469
292.578654	12484.469327	28.336487
292.731945	12502.446933	28.341504
293.145399	12519.502153	28.346522
293.177313	12541.193759	28.351540
293.427150	12555.894940	28.356557
293.834919	12570.872563	28.361575
293.945366	12597.427038	28.366592
293.909423	12619.626386	28.371610
294.749499	12629.984485	28.376628
294.974401	12665.553143	28.381645
295.427951	12682.515223	28.386663
295.646018	12698.274491	28.391680
295.670249	12718.520930	28.396698
296.057226	12732.449442	28.401716
296.473184	12768.706889	28.406733
296.752895	12781.565823	28.411751
297.218227	12797.443426	28.416768
297.190804	12829.555692	28.421786
297.376761	12844.013985	28.426804
297.533841	12866.473263	28.431821
298.498725	12885.033995	28.436839
298.987398	12912.158321	28.441856
298.913259	12924.554310	28.446874
299.079188	12940.951236	28.451892
299.534466	12958.026785	28.456909
299.820101	12967.822867	28.461927
300.242714	12994.331046	28.466944
300.232634	13005.433688	28.471962
300.788758	13013.845487	28.476980
300.882776	13036.890652	28.481997
301.154059	13052.794320	28.487015
301.449384	13069.302336	28.492032
301.806624	13091.118905	28.497050
301.676345	13103.021598	28.502068
302.170098	13130.605622	28.507085
302.320713	13150.577951	28.512103
302.497634	13166.127003	28.517120
302.852789	13198.608478	28.522138
303.482930	13220.501398	28.527156
303.290955	13248.629358	28.532173
303.583830	13280.027593	28.537191
304.488007	13299.003870	28.542208
304.087932	13322.725358	28.547226
304.777948	13341.694582	28.552244
305.602097	13371.162757	28.557261
305.681059	13384.302824	28.562279
306.420394	13410.600084	28.567296
306.675617	13429.302545	28.572314
307.194305	13431.420034	28.577332
306.990108	13449.966896	28.582349
307.373798	13470.993187	28.587367
307.972669	13484.266338	28.592384
307.999021	13504.653662	28.597402
308.103877	13520.222860	28.602420
308.660522	13547.040710	28.607437
308.961724	13568.711173	28.612455
309.300101	13585.135362	28.617472
309.305358	13615.138247	28.622490
309.636047	13626.612000	28.627508
310.109750	13640.077779	28.632525
310.032889	13684.205801	28.637543
310.446566	13694.605222	28.642560
310.456562	13731.314971	28.647578
310.957824	13748.520852	28.652596
311.448536	13783.469558	28.657613
311.755656	13795.063955	28.662631
312.199782	13823.982786	28.667648
312.498689	13853.770447	28.672666
313.020559	13872.003758	28.677684
313.461609	13885.795076	28.682701
313.573436	13903.897715	28.687719
314.054626	13928.065216	28.692736
314.063268	13942.724043	28.697754
314.570383	13970.871492	28.702772
315.106533	13989.827541	28.707789
315.342037	14014.166645	28.712807
315.494078	14026.890093	28.717824
315.490279	14053.377588	28.722842
315.715241	14063.360888	28.727860
316.238735	14090.963679	28.732877
316.158927	14119.121848	28.737895
316.738725	14142.984931	28.742912
317.208277	14178.097164	28.747930
317.362755	14193.356189	28.752948
317.724158	14211.154659	28.757965
317.952200	14242.336948	28.762983
318.370871	14262.759571	28.768000
318.898531	14293.799378	28.773018
319.133977	14318.235083	28.778036
319.757762	14344.269287	28.783053
319.704711	14363.490356	28.788071
320.734196	14374.401371	28.793088
320.625853	14411.152719	28.798106
320.890118	14420.820824	28.803124
321.233808	14448.069419	28.808141
321.382586	14464.149194	28.813159
321.897912	14482.284978	28.818176
322.031071	14496.810214	28.823194
322.330317	14512.543614	28.828212
322.708460	14527.184358	28.833229
322.438040	14561.277237	28.838247
323.365664	14572.662309	28.843264
323.129508	14595.384483	28.848282
323.680784	14620.997707	28.853300
324.191739	14641.457539	28.858317
324.349584	14675.092051	28.863335
324.656300	14706.333125	28.868352
325.125092	14732.095720	28.873370
325.419577	14758.404165	28.878388
325.810002	14780.627285	28.883405
325.791915	14807.053741	28.888423
326.279041	14827.391662	28.893440
326.533306	14861.165053	28.898458
326.833146	14882.077798	28.903476
327.261146	14903.405939	28.908493
327.288083	14937.920061	28.913511
328.365080	14953.542491	28.918528
328.827375	14990.282641	28.923546
329.025853	14993.648040	28.928564
329.322759	15027.953750	28.933581
329.726377	15044.570352	28.938599
330.050903	15062.251338	28.943616
330.293150	15093.012066	28.948634
330.359347	15115.933942	28.953652
330.930879	15140.108770	28.958669
331.292446	15164.729758	28.963687
331.299198	15169.644746	28.968704
331.895983	15210.955992	28.973722
332.209625	15234.599929	28.978740
332.533357	15251.256757	28.983757
332.660554	15277.861668	28.988775
332.905075	15309.971608	28.993792
333.257598	15333.935515	28.998810
333.489482	15363.801634	29.003828
334.343086	15388.934153	29.008845
334.259313	15428.356867	29.013863
334.960396	15444.962468	29.018880
335.111129	15464.646008	29.023898
335.436700	15494.490553	29.028916
335.621914	15514.453732	29.033933
335.916622	15547.479463	29.038951
336.561759	15572.071464	29.043968
336.707491	15594.545817	29.048986
337.087205	15614.839446	29.054004
337.516043	15636.537227	29.059021
337.884889	15671.544806	29.064039
338.288698	15684.391791	29.069056
339.036153	15712.184062	29.074074
339.356019	15733.122947	29.079092
339.727271	15754.274020	29.084109
339.799279	15770.156570	29.089127
340.185227	15778.780810	29.094144
340.422472	15806.607250	29.099162
340.686437	15826.518368	29.104180
341.029830	15847.258054	29.109197
341.275875	15883.465407	29.114215
341.529486	15898.471601	29.119232
341.756952	15932.656712	29.124250
342.152265	15964.935267	29.129268
342.637065	15984.562560	29.134285
342.596962	16024.070888	29.139303
343.287917	16036.917910	29.144320
343.390745	16072.359695	29.149338
343.946224	16089.795499	29.154356
344.191953	16107.011478	29.159373
344.490333	16142.960117	29.164391
344.760933	16155.701845	29.169408
344.916847	16185.269932	29.174426
345.376379	16210.306581	29.179444
346.123660	16229.310667	29.184461
346.080367	16255.929611	29.189479
346.461282	16273.002018	29.194496
346.660050	16297.832913	29.199514
346.945156	16330.910666	29.204532
347.538777	16355.394147	29.209549
347.700681	16389.942558	29.214567
348.128295	16413.217819	29.219584
348.531296	16441.697260	29.224602
348.722757	16478.881197	29.229620
349.213333	16500.643983	29.234637
349.197447	16540.179484	29.239655
350.018104	16561.553549	29.244672
350.197243	16595.697589	29.249690
350.621604	16621.038598	29.254708
351.343710	16644.216578	29.259725
351.405592	16677.524276	29.264743
351.639548	16700.302363	29.269760
352.367919	16732.993875	29.274778
352.579288	16759.182135	29.279796
353.292069	16782.131714	29.284813
353.193215	16816.136217	29.289831
353.867503	16841.371571	29.294848
354.238930	16858.477680	29.299866
354.428013	16883.788675	29.304884
355.050060	16901.647804	29.309901
355.352205	16933.839637	29.314919
355.725661	16955.860430	29.319936
355.699979	16980.540341	29.324954
356.060605	17019.127205	29.329972
356.700384	17028.171950	29.334989
356.967112	17064.693728	29.340007
357.227029	17099.402368	29.345024
357.850463	17123.478516	29.350042
358.016337	17157.457242	29.355060
358.210799	17184.206992	29.360077
358.540192	17208.812711	29.365095
358.902642	17243.528327	29.370112
359.287869	17271.996375	29.375130
359.546524	17316.765863	29.380148
360.083532	17342.313173	29.385165
360.246211	17364.372547	29.390183
360.829601	17389.901219	29.395200
361.195580	17414.329366	29.400218
361.575523	17451.290397	29.405236
362.330997	17471.407467	29.410253
362.614246	17499.998401	29.415271
362.694415	17526.523283	29.420288
363.146022	17537.777985	29.425306
363.451619	17570.512750	29.430324
364.152286	17590.973226	29.435341
364.015721	17623.506989	29.440359
364.595424	17647.297932	29.445376
364.927831	17662.409338	29.450394
365.013926	17704.068293	29.455412
365.750181	17724.110033	29.460429
366.138309	17751.880088	29.465447
366.537302	17777.080462	29.470464
367.239946	17806.223606	29.475482
367.394467	17831.073579	29.480500
367.888344	17850.476163	29.485517
367.918046	17873.154097	29.490535
368.215553	17890.536765	29.495552
368.803631	17912.679370	29.500570
368.852076	17934.105778	29.505588
369.250370	17950.475544	29.510605
369.239593	17980.675028	29.515623
369.422532	18013.888124	29.520640
369.976146	18039.235132	29.525658
370.088138	18080.783547	29.530676
370.434855	18112.870974	29.535693
370.930616	18135.182068	29.540711
371.087081	18171.782854	29.545728
371.601105	18209.699185	29.550746
372.121941	18236.338282	29.555764
372.296384	18266.140320	29.560781
372.722381	18303.943744	29.565799
373.421823	18339.734603	29.570816
373.868268	18370.672562	29.575834
373.816690	18410.316152	29.580852
374.760568	18443.028970	29.585869
375.053107	18466.520220	29.590887
375.468532	18491.130940	29.595904
376.180878	18522.878035	29.600922
376.195131	18549.486394	29.605940
377.127394	18577.940236	29.610957
377.215264	18600.157087	29.615975
377.661096	18633.636893	29.620992
377.854288	18650.370774	29.626010
378.005201	18679.267823	29.631028
378.807633	18707.877375	29.636045
378.968718	18739.566354	29.641063
379.545622	18765.446617	29.646080
380.038565	18786.321303	29.651098
380.155055	18827.933892	29.656116
380.525067	18846.957713	29.661133
381.001178	18871.940461	29.666151
381.041204	18919.223948	29.671168
381.479813	18937.795102	29.676186
381.536097	18976.254000	29.681204
382.150304	19009.184872	29.686221
382.631324	19042.386940	29.691239
382.971170	19078.221558	29.696256
383.392359	19104.829665	29.701274
383.453053	19147.467554	29.706292
384.102033	19168.124559	29.711309
384.718548	19209.072028	29.716327
384.853123	19237.501366	29.721344
385.368909	19277.767275	29.726362
385.576151	19314.109914	29.731380
386.117370	19340.916092	29.736397
386.474380	19385.409996	29.741415
387.049944	19408.570377	29.746432
387.614843	19445.177298	29.751450
388.046739	19474.585737	29.756468
388.172508	19490.970589	29.761485
388.646827	19529.404137	29.766503
389.150413	19557.831279	29.771520
389.619741	19583.708543	29.776538
389.919394	19611.155802	29.781556
390.570216	19637.685761	29.786573
390.854379	19663.852350	29.791591
391.119919	19690.288502	29.796608
391.823599	19712.116399	29.801626
391.871434	19744.380974	29.806644
392.077694	19766.575048	29.811661
392.656594	19799.563772	29.816679
392.790763	19828.779313	29.821696
393.109130	19854.711936	29.826714
393.532270	19888.305217	29.831732
393.622107	19921.770844	29.836749
394.507719	19954.625553	29.841767
394.273546	19986.494243	29.846784
394.714271	20012.774205	29.851802
395.224416	20045.185144	29.856820
395.243990	20085.617101	29.861837
395.914853	20107.685860	29.866855
396.226982	20153.459971	29.871872
396.616594	20180.533806	29.876890
397.112681	20218.124997	29.881908
397.306588	20261.760584	29.886925
398.132030	20295.579774	29.891943
398.265181	20329.061115	29.896960
398.915242	20364.142389	29.901978
399.326775	20400.814619	29.906996
399.849451	20425.441968	29.912013
400.303923	20461.101330	29.917031
400.174430	20490.066825	29.922048
400.995905	20524.807891	29.927066
401.573134	20566.127806	29.932084
401.732328	20600.242341	29.937101
402.218848	20635.264532	29.942119
402.808516	20663.652498	29.947136
403.217781	20697.227620	29.952154
403.510829	20730.090472	29.957172
404.056058	20753.628250	29.962189
404.615139	20777.423919	29.967207
405.133036	20818.421595	29.972224
405.182501	20834.489285	29.977242
406.084710	20861.939773	29.982260
406.594286	20891.755657	29.987277
406.836717	20924.179488	29.992295
407.037675	20954.756066	29.997312
407.674882	20970.077022	30.002330
407.915183	20999.502497	30.007348
408.053446	21032.918169	30.012365
408.396771	21070.113992	30.017383
408.402394	21106.293631	30.022400
409.019427	21134.781927	30.027418
409.686319	21177.808683	30.032436
410.020528	21203.426999	30.037453
410.579575	21246.951099	30.042471
410.733085	21286.498154	30.047488
411.376991	21309.739725	30.052506
411.647420	21336.168193	30.057524
411.738493	21378.321074	30.062541
412.336938	21414.707571	30.067559
412.937366	21457.675089	30.072576
413.279529	21488.183538	30.077594
413.733645	21535.142526	30.082612
414.093154	21568.122150	30.087629
414.737706	21600.468116	30.092647
414.909260	21648.141143	30.097664
415.479433	21670.999651	30.102682
415.623548	21706.580564	30.107700
415.895238	21744.847729	30.112717
416.729746	21779.131970	30.117735
416.886001	21826.349193	30.122752
417.327967	21862.822469	30.127770
417.819223	21900.326759	30.132788
418.438966	21929.235369	30.137805
419.003787	21974.117988	30.142823
418.847742	21994.260496	30.147840
419.505644	22036.597145	30.152858
420.151085	22069.864705	30.157876
420.128957	22106.565105	30.162893
421.012336	22143.025852	30.167911
421.091186	22179.749119	30.172928
421.591683	22201.672222	30.177946
421.495059	22242.950080	30.182964
422.174881	22279.244554	30.187981
422.547563	22303.795403	30.192999
422.876131	22344.232081	30.198016
423.320058	22385.747228	30.203034
423.682407	22432.987221	30.208052
424.315168	22474.152816	30.213069
424.583376	22501.266235	30.218087
424.844894	22538.516667	30.223104
425.383902	22587.724122	30.228122
425.876110	22626.380951	30.233140
426.144840	22661.333005	30.238157
426.768003	22696.291126	30.243175
427.203284	22741.339130	30.248192
427.715308	22778.411445	30.253210
428.398864	22813.722490	30.258228
428.529577	22863.559673	30.263245
429.166858	22896.150579	30.268263
429.647032	22934.846369	30.273280
430.155186	22963.100313	30.278298
430.482148	23005.836330	30.283316
430.769756	23047.659648	30.288333
431.352566	23077.654915	30.293351
431.855434	23112.646416	30.298368
432.120782	23148.905692	30.303386
432.753931	23185.542552	30.308404
433.140966	23220.810478	30.313421
433.732556	23250.295261	30.318439
434.183461	23293.424635	30.323456
434.376378	23328.095725	30.328474
434.892812	23375.293912	30.333492
435.191794	23408.044284	30.338509
435.903957	23438.878199	30.343527
435.944838	23488.255847	30.348544
436.343266	23525.283936	30.353562
437.059535	23568.114629	30.358580
437.510250	23611.706880	30.363597
438.286331	23654.975741	30.368615
438.511806	23688.246589	30.373632
438.560881	23721.218690	30.378650
439.503569	23751.359014	30.383668
440.015876	23794.615112	30.388685
440.459948	23826.560112	30.393703
440.860365	23871.613720	30.398720
441.009405	23907.281998	30.403738
441.485896	23941.710285	30.408756
441.839949	23986.727715	30.413773
442.653120	24019.040928	30.418791
443.212863	24065.200943	30.423808
443.221365	24101.340742	30.428826
444.056323	24130.528150	30.433844
444.079190	24169.983677	30.438861
444.701801	24209.239118	30.443879
445.190516	24248.488421	30.448896
445.437671	24282.794496	30.453914
446.295067	24317.939541	30.458932
446.019220	24356.933985	30.463949
446.946461	24394.571903	30.468967
447.085474	24438.730372	30.473984
447.494469	24477.204889	30.479002
448.340433	24518.026319	30.484020
448.475913	24555.240508	30.489037
448.959798	24596.232434	30.494055
449.551542	24639.471216	30.499072
449.745298	24678.972177	30.504090
450.500572	24713.119329	30.509108
450.839671	24771.880398	30.514125
451.552419	24793.626631	30.519143
451.958832	24828.841050	30.524160
452.106751	24872.295800	30.529178
452.571673	24886.601661	30.534196
452.836953	24932.923139	30.539213
453.495149	24961.131907	30.544231
453.836854	25006.049974	30.549248
454.318538	25039.539685	30.554266
454.830338	25081.080123	30.559284
454.984484	25128.045035	30.564301
455.509082	25165.694508	30.569319
455.952161	25207.678742	30.574336
456.531693	25246.136226	30.579354
456.754271	25287.352833	30.584372
456.984607	25326.562201	30.589389
457.877416	25370.932666	30.594407
458.058765	25428.129221	30.599424
458.727797	25465.354867	30.604442
459.343444	25496.877160	30.609460
459.603684	25537.914654	30.614477
460.000125	25577.567083	30.619495
460.535992	25632.198043	30.624512
460.967990	25669.904950	30.629530
461.583281	25711.726284	30.634548
461.870107	25762.014469	30.639565
462.495153	25802.642101	30.644583
462.952158	25852.634277	30.649600
463.485421	25895.409604	30.654618
464.159274	25941.022710	30.659636
464.331831	25985.192215	30.664653
465.267295	26022.993219	30.669671
465.514742	26054.829811	30.674688
465.795210	26100.704005	30.679706
466.930110	26125.372363	30.684724
467.202652	26170.317530	30.689741
467.926825	26205.538964	30.694759
468.210230	26249.047315	30.699776
468.668378	26297.652681	30.704794
469.176792	26324.743447	30.709812
469.160581	26365.260873	30.714829
469.843596	26410.769612	30.719847
470.287957	26441.766813	30.724864
470.522243	26488.924049	30.729882
471.171918	26525.678879	30.734900
471.578297	26579.558288	30.739917
472.181505	26613.226525	30.744935
472.842125	26661.531284	30.749952
472.887178	26695.825142	30.754970
473.603992	26736.963426	30.759988
473.938009	26786.568581	30.765005
474.159515	26826.413705	30.770023
474.549772	26876.930912	30.775040
474.764029	26926.004254	30.780058
475.625891	26969.481784	30.785076
475.982807	27027.061506	30.790093
476.503527	27072.131979	30.795111
476.970994	27130.463447	30.800128
477.668234	27178.438675	30.805146
478.396745	27215.948474	30.810164
478.640953	27263.431092	30.815181
478.976401	27306.252110	30.820199
479.754824	27346.921087	30.825216
480.080529	27395.718644	30.830234
480.651314	27435.261313	30.835252
481.308252	27487.600513	30.840269
481.357131	27523.772342	30.845287
481.907998	27568.892746	30.850304
482.287612	27618.148885	30.855322
482.790789	27652.602263	30.860340
483.455087	27699.076486	30.865357
483.686829	27742.130254	30.870375
484.199739	27783.894679	30.875392
484.436701	27829.427332	30.880410
485.006539	27868.990074	30.885428
485.570827	27914.727465	30.890445
486.202239	27957.677774	30.895463
486.676351	28006.465105	30.900480
486.878300	28054.720305	30.905498
487.565731	28093.655248	30.910516
487.700056	28152.332349	30.915533
488.227878	28199.805294	30.920551
488.714678	28244.559490	30.925568
488.786274	28304.162346	30.930586
489.431207	28365.635927	30.935604
489.907474	28417.566161	30.940621
490.500299	28474.584797	30.945639
491.041370	28526.286954	30.950656
491.468007	28580.714989	30.955674
492.135827	28624.146751	30.960692
492.767369	28689.791147	30.965709
493.151441	28748.633986	30.970727
493.914377	28792.580434	30.975744
493.892872	28856.301825	30.980762
495.000850	28900.169365	30.985780
495.324708	28953.255840	30.990797
495.374757	29008.599330	30.995815
496.383257	29063.219675	31.000832
496.633229	29124.546754	31.005850
497.494207	29167.629265	31.010868
497.937130	29228.249637	31.015885
498.362792	29278.752179	31.020903
498.971678	29329.063648	31.025920
499.046660	29379.391046	31.030938
499.636623	29438.082247	31.035956
500.585677	29488.848983	31.040973
500.980126	29548.620344	31.045991
501.553180	29591.073231	31.051008
502.300766	29650.347966	31.056026
502.708022	29698.232993	31.061044
503.475018	29742.490345	31.066061
503.699522	29788.408760	31.071079
504.544849	29841.039348	31.076096
504.613859	29885.879500	31.081114
505.297887	29929.289738	31.086132
505.757267	29989.941571	31.091149
506.188486	30043.243898	31.096167
506.978453	30083.406239	31.101184
507.197936	30142.375644	31.106202
507.796011	30192.019354	31.111220
508.412809	30241.906201	31.116237
508.682237	30288.809179	31.121255
509.532158	30338.834411	31.126272
509.708044	30397.862367	31.131290
510.275604	30441.655981	31.136308
510.708628	30487.128398	31.141325
510.882022	30540.345535	31.146343
511.644587	30583.545623	31.151360
511.913610	30656.482610	31.156378
512.761559	30702.811381	31.161396
513.214710	30757.273337	31.166413
513.248134	30820.399589	31.171431
514.333606	30862.294329	31.176448
514.596724	30922.290866	31.181466
515.233947	30982.825191	31.186484
515.939761	31030.535079	31.191501
516.247567	31075.089482	31.196519
516.721777	31120.995294	31.201536
517.077838	31170.590308	31.206554
517.608048	31221.791060	31.211572
518.436985	31258.614550	31.216589
518.603171	31312.377909	31.221607
519.262131	31364.135181	31.226624
519.719779	31418.368099	31.231642
520.097639	31468.509360	31.236660
520.886269	31522.151430	31.241677
520.745171	31571.132513	31.246695
521.696118	31628.654312	31.251712
521.953265	31686.051297	31.256730
522.731245	31732.829788	31.261748
523.475391	31789.001139	31.266765
523.341232	31843.929645	31.271783
524.050538	31897.592291	31.276800
524.630902	31966.340176	31.281818
524.850425	32020.655361	31.286836
525.873831	32084.944416	31.291853
526.149532	32143.330604	31.296871
527.079628	32195.733323	31.301888
527.613072	32254.553697	31.306906
527.917758	32312.023727	31.311924
528.731805	32367.172450	31.316941
529.223030	32427.155274	31.321959
529.901987	32484.327273	31.326976
530.460279	32536.202449	31.331994
531.044419	32583.920884	31.337012
531.620608	32635.537794	31.342029
531.701841	32694.809956	31.347047
532.685648	32742.923390	31.352064
533.060122	32811.191112	31.357082
533.633648	32865.576524	31.362100
533.966497	32915.397992	31.367117
534.518718	32978.092658	31.372135
534.954450	33017.329448	31.377152
535.616268	33084.682894	31.382170
535.904356	33151.022380	31.387188
536.571545	33213.121379	31.392205
536.946976	33275.480296	31.397223
538.019339	33321.018292	31.402240
538.357641	33389.767557	31.407258
538.740323	33451.056131	31.412276
539.267169	33513.861017	31.417293
540.000568	33571.731210	31.422311
540.880483	33629.798246	31.427328
541.082591	33679.368938	31.432346
541.739553	33734.939199	31.437364
542.398514	33792.759313	31.442381
542.747787	33852.893498	31.447399
543.558561	33912.320379	31.452416
543.985926	33958.518981	31.457434
544.508578	34018.754420	31.462452
545.009730	34081.038544	31.467469
545.502899	34137.675399	31.472487
545.907082	34186.557663	31.477504
546.438103	34247.710816	31.482522
546.906834	34313.409350	31.487540
547.638239	34367.640674	31.492557
548.216893	34430.004705	31.497575
548.898520	34486.614637	31.502592
549.218619	34541.100736	31.507610
549.765463	34602.116779	31.512628
550.563871	34664.830279	31.517645
551.143694	34718.885773	31.522663
551.805582	34777.608004	31.527680
551.849297	34838.755439	31.532698
552.255855	34892.537160	31.537716
553.003081	34940.900805	31.542733
553.586324	35008.012556	31.547751
554.089514	35053.346182	31.552768
554.378200	35109.404537	31.557786
554.980154	35162.722375	31.562804
555.790719	35223.362364	31.567821
555.861676	35286.880086	31.572839
556.752331	35349.113631	31.577856
556.944302	35399.050531	31.582874
557.621654	35472.747596	31.587892
558.503122	35514.545050	31.592909
558.789914	35585.955982	31.597927
559.344912	35643.941287	31.602944
559.732804	35715.004620	31.607962
560.680383	35781.825427	31.612980
561.191254	35837.618894	31.617997
561.833694	35899.494592	31.623015
562.207281	35972.259268	31.628032
562.349817	36035.720441	31.633050
563.064148	36099.147193	31.638068
563.804424	36160.038674	31.643085
564.188595	36230.842695	31.648103
564.826971	36290.422748	31.653120
565.524545	36369.504495	31.658138
565.967128	36431.427708	31.663156
566.622730	36496.734019	31.668173
567.353661	36570.530854	31.673191
568.431994	36634.675680	31.678208
568.878298	36694.651808	31.683226
569.349280	36764.241038	31.688244
570.291516	36813.347560	31.693261
570.673419	36883.456983	31.698279
571.389036	36931.884857	31.703296
571.698962	36997.221761	31.708314
572.005087	37063.364378	31.713332
572.610773	37126.320330	31.718349
573.362106	37198.825431	31.723367
573.778685	37261.014597	31.728384
574.376779	37320.775146	31.733402
574.645653	37392.044662	31.738420
575.574437	37451.189099	31.743437
576.011769	37526.550288	31.748455
576.708259	37581.292602	31.753472
577.565385	37646.383485	31.758490
577.835077	37718.342232	31.763508
578.649558	37779.627740	31.768525
579.010066	37848.131507	31.773543
579.577415	37918.533035	31.778560
580.264162	37981.027167	31.783578
580.816559	38056.343103	31.788596
581.574384	38116.995206	31.793613
581.739352	38177.840297	31.798631
582.543353	38241.284956	31.803648
583.399233	38314.228580	31.808666
583.757725	38376.052387	31.813684
584.285524	38436.374302	31.818701
584.819125	38516.048067	31.823719
585.260826	38577.795658	31.828736
585.904394	38652.028903	31.833754
586.421627	38713.341479	31.838772
586.981073	38784.246389	31.843789
587.958043	38856.676565	31.848807
588.422136	38929.280270	31.853824
589.216446	38984.916557	31.858842
589.395111	39059.559818	31.863860
590.581678	39128.793468	31.868877
590.837073	39194.311409	31.873895
591.431653	39262.216710	31.878912
592.165484	39316.131010	31.883930
592.647261	39387.066889	31.888948
593.359434	39429.832598	31.893965
593.984645	39492.275790	31.898983
593.909311	39547.552600	31.904000
594.877350	39611.994488	31.909018
595.515518	39669.205474	31.914036
596.065462	39734.733431	31.919053
596.458083	39800.698027	31.924071
597.031366	39866.686634	31.929088
597.616954	39933.541552	31.934106
598.162422	40002.663601	31.939124
598.516838	40067.041302	31.944141
599.217537	40132.350012	31.949159
600.191056	40212.043593	31.954176
600.706851	40270.492070	31.959194
601.072091	40349.339839	31.964212
601.449370	40421.461868	31.969229
602.497194	40505.646089	31.974247
603.185129	40575.930542	31.979264
603.588264	40638.947881	31.984282
603.850394	40719.402203	31.989300
604.728363	40773.931469	31.994317
605.099741	40848.452235	31.999335
606.082814	40931.477897	32.004352
606.327517	40993.730268	32.009370
606.456056	41089.349013	32.014388
607.848927	41159.626393	32.019405
608.405064	41243.342858	32.024423
609.023448	41323.261003	32.029440
609.837569	41383.261087	32.034458
610.384985	41457.976173	32.039476
611.025210	41529.440245	32.044493
612.019494	41603.371651	32.049511
612.115262	41676.372296	32.054528
613.268561	41741.583404	32.059546
613.598216	41820.664326	32.064564
614.275395	41893.089753	32.069581
614.631762	41965.445413	32.074599
615.570549	42038.421661	32.079616
616.426942	42102.871783	32.084634
617.050019	42177.488849	32.089652
617.471546	42243.880437	32.094669
618.021139	42314.699524	32.099687
618.409630	42386.852607	32.104704
619.081110	42462.507836	32.109722
619.632374	42543.916750	32.114740
620.025542	42616.186765	32.119757
621.416857	42693.002512	32.124775
621.867051	42765.557294	32.129792
622.606275	42828.311774	32.134810
623.098550	42914.357446	32.139828
623.681076	42977.049948	32.144845
624.454446	43053.331647	32.149863
624.831410	43127.143924	32.154880
625.571878	43199.390313	32.159898
626.038719	43282.884463	32.164916
626.596097	43349.153318	32.169933
627.293749	43421.672867	32.174951
627.724143	43504.103691	32.179968
628.569742	43564.699194	32.184986
629.135999	43648.235360	32.190004
629.700647	43721.898952	32.195021
630.642280	43800.937540	32.200039
630.986705	43879.453252	32.205056
631.505937	43953.646245	32.210074
631.784510	44039.018863	32.215092
632.727950	44106.224284	32.220109
633.680147	44177.122753	32.225127
633.988095	44241.825718	32.230144
634.733697	44311.798997	32.235162
635.366737	44379.912438	32.240180
636.180916	44445.953236	32.245197
636.963900	44509.205006	32.250215
637.200890	44579.228695	32.255232
638.129489	44646.097492	32.260250
638.613358	44715.689307	32.265268
639.423788	44781.040396	32.270285
639.981122	44847.289292	32.275303
640.562774	44927.238416	32.280320
641.148769	44993.893576	32.285338
641.612806	45073.875411	32.290356
642.311753	45146.458249	32.295373
643.144852	45226.594394	32.300391
643.563499	45301.144057	32.305408
644.341403	45368.630837	32.310426
644.994796	45453.471047	32.315444
645.442063	45519.693151	32.320461
646.376077	45589.949468	32.325479
646.863269	45678.860068	32.330496
647.689357	45761.819504	32.335514
647.915841	45830.033866	32.340532
648.582409	45909.651011	32.345549
649.674213	45992.147514	32.350567
650.227939	46076.078618	32.355584
651.011281	46145.133541	32.360602
651.587201	46227.915360	32.365620
651.640580	46302.011512	32.370637
652.598210	46389.808694	32.375655
653.090664	46478.456917	32.380672
653.843169	46556.827838	32.385690
654.415922	46639.466714	32.390708
654.900410	46725.477408	32.395725
655.861364	46814.826539	32.400743
656.346020	46899.950618	32.405760
657.428642	46983.485600	32.410778
658.122936	47064.988304	32.415796
658.787752	47149.088934	32.420813
659.539110	47233.879851	32.425831
660.090291	47315.644154	32.430848
661.101592	47386.668056	32.435866
661.689722	47482.682262	32.440884
662.178379	47550.256241	32.445901
663.160577	47613.245422	32.450919
663.557877	47708.869157	32.455936
664.414906	47782.838117	32.460954
664.840135	47863.024454	32.465972
665.400771	47943.450849	32.470989
666.135295	48032.202054	32.476007
666.498235	48123.589028	32.481024
667.569307	48198.496894	32.486042
668.342326	48271.009944	32.491060
668.575450	48359.930888	32.496077
669.296736	48439.489558	32.501095
670.043632	48533.679448	32.506112
670.449947	48620.472741	32.511130
670.835993	48706.142289	32.516148
671.676266	48794.683722	32.521165
672.509587	48875.849009	32.526183
673.003020	48976.873274	32.531200
673.965624	49053.179438	32.536218
674.256803	49144.381014	32.541236
674.782303	49233.623997	32.546253
675.795014	49334.333677	32.551271
676.450205	49427.377694	32.556288
677.148892	49505.077930	32.561306
677.756683	49585.481298	32.566324
678.704803	49670.657884	32.571341
679.138653	49740.086831	32.576359
679.511756	49826.205683	32.581376
680.248553	49913.537601	32.586394
680.919623	49994.393337	32.591412
681.472664	50082.100687	32.596429
682.554607	50180.371321	32.601447
683.076906	50255.311665	32.606464
683.737131	50337.418234	32.611482
684.367231	50423.257185	32.616500
685.043307	50517.193703	32.621517
685.954977	50596.871927	32.626535
686.463869	50696.623427	32.631552
687.239659	50781.403856	32.636570
687.786036	50871.724871	32.641588
688.622976	50969.458863	32.646605
689.529872	51047.762580	32.651623
690.211939	51144.657614	32.656640
690.909632	51231.000659	32.661658
691.688630	51322.315008	32.666676
692.262513	51413.063568	32.671693
693.048550	51491.483829	32.676711
693.363307	51591.663719	32.681728
693.810412	51678.833566	32.686746
695.004510	51765.545404	32.691764
695.821099	51862.655508	32.696781
696.371025	51951.167827	32.701799
696.848316	52052.296097	32.706816
697.573433	52151.855035	32.711834
698.670840	52243.190523	32.716852
699.220960	52334.465350	32.721869
699.729690	52415.973997	32.726887
700.639696	52524.867056	32.731904
701.424589	52616.287575	32.736922
702.386268	52708.664850	32.741940
702.622882	52804.232959	32.746957
703.522949	52900.209844	32.751975
704.056454	52987.725037	32.756992
705.176828	53086.414662	32.762010
705.887665	53168.790151	32.767028
706.271424	53272.953850	32.772045
707.128124	53354.345660	32.777063
707.529705	53466.714499	32.782080
708.176338	53550.378450	32.787098
709.233751	53643.862590	32.792116
709.574510	53742.305396	32.797133
710.366105	53840.124437	32.802151
711.163249	53942.662719	32.807168
711.839351	54045.866016	32.812186
712.642625	54145.049372	32.817204
713.255863	54246.861471	32.822221
714.424108	54341.290968	32.827239
714.996797	54438.144580	32.832256
715.648889	54529.589654	32.837274
716.688138	54623.789107	32.842292
717.234195	54717.002783	32.847309
717.950905	54808.008803	32.852327
718.327687	54908.713472	32.857344
719.260912	55004.360254	32.862362
720.049999	55091.975206	32.867380
720.653912	55197.401629	32.872397
721.620378	55283.193610	32.877415
722.236656	55386.698141	32.882432
723.167156	55485.071027	32.887450
724.078512	55571.650569	32.892468
724.430928	55668.331801	32.897485
725.159039	55751.397637	32.902503
725.614865	55846.470304	32.907520
726.177747	55920.003868	32.912538
727.266511	56001.861070	32.917556
727.720348	56097.396540	32.922573
728.802907	56180.670929	32.927591
729.538801	56282.062466	32.932608
729.911702	56364.690427	32.937626
730.416300	56454.222535	32.942644
731.112299	56554.939610	32.947661
731.765953	56645.566384	32.952679
732.750814	56740.720101	32.957696
733.386180	56836.020551	32.962714
734.423145	56926.022793	32.967732
734.683593	57033.740087	32.972749
735.196059	57128.499856	32.977767
736.116921	57236.475510	32.982784
736.720200	57341.685893	32.987802
737.618436	57445.388283	32.992820
738.172740	57549.432472	32.997837
739.072849	57648.870067	33.002855
739.570588	57759.086064	33.007872
740.462968	57868.485374	33.012890
741.541672	57980.944672	33.017908
742.075090	58092.009718	33.022925
742.612336	58182.074986	33.027943
743.584460	58299.356526	33.032960
744.346048	58414.746102	33.037978
745.206369	58506.503585	33.042996
746.016689	58628.414489	33.048013
746.744932	58722.962815	33.053031
747.717004	58826.919225	33.058048
748.389797	58938.433540	33.063066
749.428878	59037.709657	33.068084
750.172925	59144.031099	33.073101
750.688213	59237.959801	33.078119
751.715375	59348.115871	33.083136
752.237391	59446.266106	33.088154
753.295830	59544.580884	33.093172
754.013299	59648.305556	33.098189
754.544864	59752.326950	33.103207
755.267558	59863.029144	33.108224
755.830421	59970.054816	33.113242
756.806698	60061.326170	33.118260
757.349915	60177.640416	33.123277
758.430212	60286.907978	33.128295
759.013725	60385.393871	33.133312
759.689592	60496.973131	33.138330
760.266553	60607.633962	33.143348
760.895748	60725.751036	33.148365
762.013941	60827.260215	33.153383
762.821133	60939.325801	33.158400
763.576574	61045.933410	33.163418
764.568530	61154.822055	33.168436
765.254474	61273.261573	33.173453
766.207302	61367.981002	33.178471
766.989688	61476.526796	33.183488
767.682431	61580.840569	33.188506
768.572487	61681.051768	33.193524
769.093921	61800.665578	33.198541
769.691933	61893.575220	33.203559
770.781390	61996.782580	33.208576
771.531266	62105.640478	33.213594
772.007599	62208.444660	33.218612
772.893380	62324.297287	33.223629
773.599804	62425.692883	33.228647
774.489156	62529.264703	33.233664
775.169752	62641.632336	33.238682
776.114194	62747.231470	33.243700
776.824328	62854.235229	33.248717
777.427963	62947.477394	33.253735
778.109170	63044.531366	33.258752
779.038699	63146.500425	33.263770
779.854896	63235.619012	33.268788
780.388690	63345.852955	33.273805
781.009942	63444.922520	33.278823
781.946756	63550.128793	33.283840
782.365924	63668.683121	33.288858
783.368243	63761.578560	33.293876
783.970842	63877.404573	33.298893
784.699139	63989.442941	33.303911
785.659956	64097.378831	33.308928
786.381245	64221.809448	33.313946
787.226580	64327.673261	33.318964
787.844554	64443.601033	33.323981
788.614664	64558.593994	33.328999
789.691459	64664.863743	33.334016
790.355749	64781.392603	33.339034
791.287759	64900.690938	33.344052
791.701938	65018.842891	33.349069
792.619941	65128.959534	33.354087
793.448811	65245.735598	33.359104
794.098245	65371.992978	33.364122
794.865444	65492.086884	33.369140
795.842349	65617.210558	33.374157
796.321469	65743.296052	33.379175
797.221394	65856.510901	33.384192
797.797685	65988.909998	33.389210
798.576122	66114.581547	33.394228
799.401944	66244.513355	33.399245
800.311199	66375.962099	33.404263
801.283041	66504.809265	33.409280
801.641771	66637.697305	33.414298
802.479648	66765.240581	33.419316
803.616618	66899.126893	33.424333
804.475820	67032.642732	33.429351
805.232273	67158.697168	33.434368
805.721962	67294.115560	33.439386
806.598599	67427.972421	33.444404
807.438668	67559.123876	33.449421
808.201952	67691.983255	33.454439
809.238470	67837.557014	33.459456
809.633534	67968.904739	33.464474
811.170373	68093.918914	33.469492
812.244125	68225.219200	33.474509
813.129541	68358.163718	33.479527
813.674339	68482.819492	33.484544
814.564375	68613.741595	33.489562
815.817570	68743.637059	33.494580
816.348869	68867.146581	33.499597
817.350735	68982.207586	33.504615
818.344092	69103.928576	33.509632
818.789839	69224.014689	33.514650
819.613058	69343.653346	33.519668
820.527106	69469.151675	33.524685
821.230680	69603.076163	33.529703
822.204784	69728.547114	33.534720
822.894893	69852.782191	33.539738
823.700314	69982.929988	33.544756
824.477929	70112.141028	33.549773
825.055403	70239.558549	33.554791
825.903544	70363.606046	33.559808
826.529138	70495.784837	33.564826
827.554879	70628.581174	33.569844
828.544051	70759.948983	33.574861
828.973181	70896.936852	33.579879
830.182263	71016.830877	33.584896
830.788596	71141.390789	33.589914
831.921962	71267.135274	33.594932
832.318593	71378.597369	33.599949
833.026894	71496.641895	33.604967
834.147603	71627.177500	33.609984
834.756924	71765.652420	33.615002
835.663316	71885.278832	33.620020
836.523376	72011.218297	33.625037
837.278163	72134.285958	33.630055
838.205137	72260.544640	33.635072
838.764054	72398.228821	33.640090
839.804523	72523.091670	33.645108
840.501681	72658.876457	33.650125
841.135307	72795.159541	33.655143
842.097156	72925.305538	33.660160
842.951501	73070.691977	33.665178
843.659162	73209.001739	33.670196
844.485276	73340.804273	33.675213
845.094748	73491.932024	33.680231
846.331578	73626.514214	33.685248
847.043736	73781.098952	33.690266
847.566236	73924.528538	33.695284
848.433468	74066.934431	33.700301
849.260705	74214.533823	33.705319
850.337442	74359.190052	33.710336
851.189106	74502.625900	33.715354
852.165879	74659.108340	33.720372
853.232122	74797.115853	33.725389
853.829832	74954.112125	33.730407
855.100757	75089.677969	33.735424
855.855243	75241.698208	33.740442
856.413292	75385.612124	33.745460
857.751760	75531.466090	33.750477
858.153872	75687.753618	33.755495
859.521839	75823.851855	33.760512
859.791131	75966.451154	33.765530
860.818590	76117.338075	33.770548
861.705169	76268.831216	33.775565
862.217018	76423.360105	33.780583
863.376806	76585.195829	33.785600
863.950000	76727.351280	33.790618
865.250078	76895.117940	33.795636
865.901559	77037.996141	33.800653
866.925714	77198.119343	33.805671
868.291773	77344.600544	33.810688
868.795781	77501.276142	33.815706
869.240844	77647.158939	33.820724
870.628755	77804.930245	33.825741
871.122421	77957.910416	33.830759
872.679920	78097.419598	33.835776
873.455033	78247.483447	33.840794
874.701924	78401.619826	33.845812
875.360076	78541.824509	33.850829
875.710039	78701.766347	33.855847
876.803994	78839.212424	33.860864
877.660241	78995.966725	33.865882
878.706481	79145.662798	33.870900
879.842409	79290.347664	33.875917
880.365149	79452.347438	33.880935
881.126876	79586.076498	33.885952
882.157407	79744.553119	33.890970
883.090137	79888.794656	33.895988
884.030780	80040.279064	33.901005
884.554359	80193.503532	33.906023
885.495780	80335.013628	33.911040
886.664184	80482.155266	33.916058
887.408033	80640.938613	33.921076
888.514334	80783.999453	33.926093
889.225163	80924.267137	33.931111
890.511325	81071.488011	33.936128
890.967405	81199.988365	33.941146
891.774892	81334.795636	33.946164
892.787066	81472.821616	33.951181
893.400582	81621.833778	33.956199
894.122861	81765.135099	33.961216
895.093419	81911.932777	33.966234
895.897258	82070.083499	33.971252
897.218915	82202.381456	33.976269
897.440443	82359.808020	33.981287
898.826208	82498.645153	33.986304
899.685672	82659.859177	33.991322
900.492364	82805.557191	33.996340
901.443152	82953.857919	34.001357
902.311123	83103.647451	34.006375
903.114171	83265.944284	34.011392
904.227395	83418.561381	34.016410
905.062218	83567.334444	34.021428
906.319606	83716.386567	34.026445
906.812717	83886.109976	34.031463
907.653770	84037.162768	34.036480
908.785259	84200.449487	34.041498
909.635843	84359.348454	34.046516
910.548987	84505.817824	34.051533
911.252763	84676.727002	34.056551
912.678605	84839.469680	34.061568
913.682216	84989.248973	34.066586
914.418068	85152.677408	34.071604
915.468937	85299.445365	34.076621
916.324891	85467.892786	34.081639
917.359110	85625.169167	34.086656
918.268860	85774.772868	34.091674
919.004893	85933.157333	34.096692
920.371680	86087.433157	34.101709
920.957973	86249.679079	34.106727
921.971393	86406.793297	34.111744
923.079702	86565.474819	34.116762
923.447031	86725.267088	34.121780
924.430800	86884.072598	34.126797
925.503280	87060.696555	34.131815
926.313420	87216.774049	34.136832
927.672808	87373.710945	34.141850
928.539795	87540.937439	34.146868
929.543852	87698.378214	34.151885
930.336873	87855.753686	34.156903
931.140752	88009.983308	34.161920
932.102916	88177.888326	34.166938
932.703751	88347.183218	34.171956
933.874733	88516.625505	34.176973
934.720204	88680.136215	34.181991
935.622169	88845.708087	34.187008
937.113383	89008.468770	34.192026
937.866843	89164.796266	34.197044
939.033001	89327.188869	34.202061
939.803985	89499.767288	34.207079
940.499263	89652.291471	34.212096
941.422098	89817.866626	34.217114
942.186875	89991.696356	34.222132
943.334021	90155.546987	34.227149
944.357528	90327.583303	34.232167
945.138117	90494.787826	34.237184
946.474763	90643.497223	34.242202
946.834657	90814.020235	34.247220
948.176680	90972.876013	34.252237
948.652248	91146.825193	34.257255
950.035292	91315.347142	34.262272
951.215578	91474.270935	34.267290
951.970893	91631.107817	34.272308
953.056340	91772.853041	34.277325
953.841418	91928.680589	34.282343
954.904056	92082.729026	34.287360
955.940387	92233.377640	34.292378
956.918573	92391.524382	34.297396
957.904094	92545.778384	34.302413
958.814518	92709.014536	34.307431
959.474567	92862.653445	34.312448
960.900037	93016.407269	34.317466
961.565670	93185.801363	34.322484
962.962850	93329.080143	34.327501
963.054630	93487.931232	34.332519
964.148542	93649.187468	34.337536
965.263736	93814.593517	34.342554
965.981418	93983.528774	34.347572
966.784783	94146.539016	34.352589
967.704047	94321.950264	34.357607
968.883467	94500.674568	34.362624
969.774214	94666.262709	34.367642
970.991083	94840.039622	34.372660
971.590122	95011.198025	34.377677
972.586293	95177.677346	34.382695
973.503409	95364.895535	34.387712
974.536324	95535.346472	34.392730
975.126754	95723.900073	34.397748
976.093888	95904.600311	34.402765
977.342331	96089.363685	34.407783
978.224196	96266.086247	34.412800
979.538896	96449.062514	34.417818
980.128690	96639.895744	34.422836
981.377230	96815.668973	34.427853
982.502382	97002.333301	34.432871
983.397867	97190.606971	34.437888
984.335965	97364.897064	34.442906
985.414321	97555.738772	34.447924
986.466538	97740.673392	34.452941
987.350605	97927.612363	34.457959
988.287315	98115.265722	34.462976
989.591937	98296.098322	34.467994
990.578990	98487.323035	34.473012
991.381329	98665.246828	34.478029
992.638347	98852.365211	34.483047
993.875927	99038.013065	34.488064
994.935265	99223.235914	34.493082
995.700851	99411.838844	34.498100
997.109493	99582.001844	34.503117
998.301254	99763.711940	34.508135
998.725833	99949.234963	34.513152
1000.071765	100117.392243	34.518170
1000.951148	100303.222508	34.523188
1001.827455	100478.734505	34.528205
1003.314092	100656.172835	34.533223
1004.150800	100847.699708	34.538240
1005.242048	101022.280815	34.543258
1006.127898	101199.885558	34.548276
1007.070057	101368.010166	34.553293
1008.240172	101552.022216	34.558311
1008.958715	101732.418881	34.563328
1010.264576	101915.822233	34.568346
1011.254600	102095.150802	34.573364
1011.970221	102274.950215	34.578381
1013.336995	102460.449512	34.583399
1014.164855	102635.414327	34.588416
1015.517857	102822.653428	34.593434
1016.284931	103005.248104	34.598452
1017.091988	103173.121823	34.603469
1018.265097	103354.163780	34.608487
1019.196254	103523.367962	34.613504
1020.495795	103687.066680	34.618522
1020.950080	103851.425424	34.623540
1021.816416	104036.702074	34.628557
1022.913058	104200.348898	34.633575
1023.584208	104388.459168	34.638592
1024.789965	104563.323743	34.643610
1025.430799	104746.477016	34.648628
1026.495961	104933.892794	34.653645
1027.706785	105121.881074	34.658663
1028.569420	105305.533482	34.663680
1029.622381	105490.789501	34.668698
1030.333180	105690.947068	34.673716
1031.439607	105882.276307	34.678733
1032.510054	106075.943316	34.683751
1033.364631	106264.555884	34.688768
1034.332917	106467.526470	34.693786
1035.217346	106672.576979	34.698804
1036.693049	106869.741820	34.703821
1037.959244	107074.339651	34.708839
1038.791880	107271.233803	34.713856
1040.065735	107467.942453	34.718874
1040.981311	107678.289947	34.723892
1042.173818	107869.201203	34.728909
1043.352502	108062.712707	34.733927
1044.391069	108272.588521	34.738944
1045.182629	108477.098179	34.743962
1046.228173	108676.665391	34.748980
1047.236449	108877.468912	34.753997
1048.510805	109076.177897	34.759015
1049.352757	109295.214287	34.764032
1050.493192	109493.530460	34.769050
1051.302806	109700.326427	34.774068
1052.573852	109897.851255	34.779085
1053.583589	110103.565811	34.784103
1054.677702	110320.402636	34.789120
1056.053336	110532.697659	34.794138
1056.954004	110732.759927	34.799156
1058.072133	110945.721438	34.804173
1059.182950	111151.655170	34.809191
1060.017198	111367.871844	34.814208
1061.294994	111579.823767	34.819226
1062.127231	111780.665046	34.824244
1063.269540	111993.377294	34.829261
1064.067986	112209.593807	34.834279
1065.357381	112427.441069	34.839296
1066.651165	112638.093608	34.844314
1067.268881	112860.349937	34.849332
1068.522961	113072.570568	34.854349
1069.964557	113277.021182	34.859367
1071.133488	113509.073200	34.864384
1072.313952	113714.444343	34.869402
1073.274815	113917.205463	34.874420
1074.061755	114131.779132	34.879437
1075.288355	114338.654850	34.884455
1076.395416	114561.793975	34.889472
1077.696039	114768.812648	34.894490
1078.561199	114977.501201	34.899508
1079.592397	115195.412685	34.904525
1080.836847	115409.236271	34.909543
1081.918079	115622.416953	34.914560
1082.965861	115835.288019	34.919578
1084.193451	116044.950773	34.924596
1085.177383	116257.151370	34.929613
1086.345283	116464.255044	34.934631
1087.010432	116678.703426	34.939648
1088.421126	116894.968726	34.944666
1089.064412	117109.436619	34.949684
1090.355674	117303.627405	34.954701
1091.452042	117499.600279	34.959719
1092.204043	117715.866630	34.964736
1093.433261	117912.276496	34.969754
1094.764371	118119.694574	34.974772
1095.363935	118324.346090	34.979789
1096.617158	118544.337088	34.984807
1097.837896	118755.097803	34.989824
1099.060994	118957.724677	34.994842
1099.714709	119177.806919	34.999860
1100.701388	119388.180093	35.004877
1102.123094	119607.213588	35.009895
1103.082265	119835.790946	35.014912
1104.475761	120052.766958	35.019930
1105.160188	120265.097180	35.024948
1106.451247	120492.218210	35.029965
1107.672623	120708.074373	35.034983
1108.369886	120936.031978	35.040000
1109.918165	121162.963591	35.045018
1110.499907	121388.067180	35.050036
1111.808283	121622.151174	35.055053
1112.963843	121839.382436	35.060071
1113.967600	122076.080228	35.065088
1114.711828	122308.488727	35.070106
1116.145454	122544.967104	35.075124
1116.979178	122785.373765	35.080141
1118.464635	123020.681428	35.085159
1119.528169	123258.392554	35.090176
1120.807381	123486.577641	35.095194
1122.431921	123724.744661	35.100212
1123.101516	123957.444428	35.105229
1124.579781	124185.373781	35.110247
1125.614489	124435.709143	35.115264
1126.962585	124656.110072	35.120282
1128.280076	124897.632273	35.125300
1128.970550	125140.134556	35.130317
1130.400171	125353.378964	35.135335
1131.386959	125599.295924	35.140352
1132.825024	125824.569984	35.145370
1134.013835	126053.131536	35.150388
1135.047552	126294.889151	35.155405
1136.631207	126523.046720	35.160423
1137.644951	126753.378835	35.165440
1138.709371	126994.705938	35.170458
1139.956486	127218.196627	35.175476
1141.026246	127454.507218	35.180493
1142.573786	127672.982967	35.185511
1143.477056	127909.033022	35.190528
1144.419447	128138.043678	35.195546
1145.464218	128366.861638	35.200564
1146.374534	128608.150711	35.205581
1147.970671	128837.159825	35.210599
1148.689587	129083.022015	35.215616
1150.068848	129318.230820	35.220634
1151.332933	129539.187539	35.225652
1151.917343	129779.233892	35.230669
1153.543493	130024.801350	35.235687
1154.701347	130265.555184	35.240704
1155.831790	130494.260384	35.245722
1157.017173	130730.639938	35.250740
1158.125168	130974.931387	35.255757
1159.654473	131201.255973	35.260775
1160.570475	131437.444454	35.265792
1161.447344	131675.808848	35.270810
1162.783147	131907.887571	35.275828
1163.944695	132148.857847	35.280845
1165.219000	132382.522089	35.285863
1166.402009	132618.206079	35.290880
1167.366038	132839.387409	35.295898
1168.718111	133061.342796	35.300916
1169.367864	133290.210799	35.305933
1170.822107	133511.290327	35.310951
1172.046792	133739.749524	35.315968
1173.104783	133957.842339	35.320986
1174.644855	134187.672419	35.326004
1175.182604	134417.859975	35.331021
1176.890425	134642.632491	35.336039
1177.907064	134870.474743	35.341056
1178.797179	135109.001631	35.346074
1180.113214	135333.323844	35.351092
1181.235665	135578.142052	35.356109
1182.214302	135811.372612	35.361127
1183.248321	136059.403907	35.366144
1184.522481	136304.303831	35.371162
1185.688298	136540.526031	35.376180
1186.546593	136789.948420	35.381197
1188.186093	137034.019924	35.386215
1189.273300	137282.824934	35.391232
1190.346328	137539.000549	35.396250
1191.735878	137777.210438	35.401268
1192.458941	138039.229316	35.406285
1193.840272	138296.424772	35.411303
1195.296299	138540.778450	35.416320
1196.008057	138792.750405	35.421338
1197.524867	139053.707657	35.426356
1198.831875	139319.177464	35.431373
1199.824204	139575.432553	35.436391
1201.265729	139837.118306	35.441408
1202.678277	140091.126884	35.446426
1203.651086	140346.262464	35.451444
1205.295918	140608.554490	35.456461
1206.288199	140864.071088	35.461479
1207.958204	141130.243028	35.466496
1209.035319	141378.204688	35.471514
1210.635074	141638.178806	35.476532
1211.585528	141894.686304	35.481549
1213.052557	142129.870361	35.486567
1214.502347	142383.331662	35.491584
1215.509379	142637.387898	35.496602
1216.749221	142880.793635	35.501620
1217.796172	143142.696360	35.506637
1219.167186	143379.540509	35.511655
1220.411648	143634.376279	35.516672
1221.604993	143883.363624	35.521690
1222.873989	144137.501493	35.526708
1223.584150	144397.262631	35.531725
1225.150858	144654.018066	35.536743
1226.332263	144909.761106	35.541760
1227.267335	145167.829387	35.546778
1228.973619	145420.344264	35.551796
1230.125651	145692.304998	35.556813
1231.429908	145941.377119	35.561831
1232.657444	146185.099153	35.566848
1233.968946	146453.412206	35.571866
1234.690427	146713.454527	35.576884
1236.172069	146968.198688	35.581901
1237.416822	147231.011723	35.586919
1238.648219	147487.589087	35.591936
1239.879558	147753.984550	35.596954
1241.186362	148008.726810	35.601972
1242.621993	148279.822940	35.606989
1243.944865	148526.233572	35.612007
1245.347231	148781.865859	35.617024
1246.737754	149036.918449	35.622042
1248.023482	149290.696440	35.627060
1248.869450	149542.227831	35.632077
1250.273771	149775.062310	35.637095
1251.734259	150016.183847	35.642112
1252.732689	150262.659605	35.647130
1254.102584	150487.019004	35.652148
1255.291730	150721.049119	35.657165
1256.607012	150959.549845	35.662183
1258.225692	151196.796975	35.667200
1258.850954	151449.328880	35.672218
1260.233367	151680.821592	35.677236
1261.213832	151925.789094	35.682253
1262.568170	152173.119024	35.687271
1263.772694	152415.350930	35.692288
1265.006085	152672.711852	35.697306
1266.640625	152916.740426	35.702324
1267.421438	153167.773900	35.707341
1268.736071	153419.152045	35.712359
1270.380675	153686.053894	35.717376
1271.297991	153940.900551	35.722394
1272.463940	154186.130830	35.727412
1273.627884	154448.385965	35.732429
1275.049744	154713.708023	35.737447
1276.286868	154979.455646	35.742464
1277.507440	155250.865333	35.747482
1278.912212	155515.079345	35.752500
1280.177211	155782.083604	35.757517
1281.366313	156043.254284	35.762535
1282.887431	156312.071835	35.767552
1283.898686	156587.559234	35.772570
1285.188921	156855.099319	35.777588
1286.503504	157136.274239	35.782605
1287.946789	157404.021035	35.787623
1288.883473	157667.527481	35.792640
1290.228691	157946.584469	35.797658
1291.890776	158230.335571	35.802676
1292.861961	158504.003243	35.807693
1293.996565	158784.635821	35.812711
1295.606050	159072.828966	35.817728
1296.768013	159347.777449	35.822746
1298.099007	159627.381129	35.827764
1299.430119	159908.432951	35.832781
1300.630433	160190.853085	35.837799
1301.879628	160478.088008	35.842816
1303.361846	160767.392409	35.847834
1304.845243	161044.011767	35.852852
1306.232290	161325.939337	35.857869
1307.553830	161613.017880	35.862887
1309.161859	161888.391578	35.867904
1310.290661	162166.294910	35.872922
1311.917795	162447.061158	35.877940
1313.063865	162729.355135	35.882957
1314.582538	163007.694359	35.887975
1316.207098	163277.897882	35.892992
1316.923232	163555.015751	35.898010
1318.528496	163830.402498	35.903028
1319.762728	164107.945815	35.908045
1321.388717	164391.896979	35.913063
1322.772957	164666.678519	35.918080
1323.804768	164943.042610	35.923098
1325.124810	165222.926176	35.928116
1326.701032	165496.513926	35.933133
1327.690798	165773.334311	35.938151
1329.147122	166044.052372	35.943168
1330.446379	166329.161347	35.948186
1331.719703	166600.649000	35.953204
1332.958488	166884.566143	35.958221
1334.561925	167163.717342	35.963239
1335.844908	167432.112449	35.968256
1336.875544	167715.066875	35.973274
1338.339282	167990.198595	35.978292
1339.544736	168251.289930	35.983309
1341.001044	168513.381821	35.988327
1342.247068	168779.710080	35.993344
1342.913328	169048.838517	35.998362
1344.485855	169325.914519	36.003380
1345.664412	169603.019246	36.008397
1346.825771	169888.846124	36.013415
1348.294083	170164.916585	36.018432
1349.083804	170451.874298	36.023450
1350.357124	170742.586144	36.028468
1351.739051	171028.941975	36.033485
1353.529906	171333.809875	36.038503
1354.814215	171632.837298	36.043520
1355.900297	171927.039127	36.048538
1357.630918	172221.466219	36.053556
1359.132589	172503.318993	36.058573
1360.224577	172815.215432	36.063591
1361.855924	173116.897925	36.068608
1362.969992	173410.558665	36.073626
1364.255617	173711.261437	36.078644
1365.766269	174016.167542	36.083661
1366.945583	174323.414645	36.088679
1368.641124	174622.672085	36.093696
1369.500139	174928.795726	36.098714
1371.088178	175228.049276	36.103732
1372.203665	175545.226202	36.108749
1373.762204	175865.923516	36.113767
1375.450825	176181.093484	36.118784
1376.572050	176489.670979	36.123802
1378.230313	176803.365055	36.128820
1379.468344	177116.660975	36.133837
1380.453201	177443.415522	36.138855
1382.382557	177751.423064	36.143872
1383.704702	178067.896582	36.148890
1384.771511	178393.463424	36.153908
1386.880849	178700.520509	36.158925
1388.085373	179031.640344	36.163943
1389.446982	179347.582236	36.168960
1390.607930	179668.509099	36.173978
1392.456586	179988.994313	36.178996
1394.037367	180308.358102	36.184013
1395.329359	180623.963912	36.189031
1396.948112	180931.724567	36.194048
1398.288698	181261.693851	36.199066
1399.839665	181569.075975	36.204084
1401.808218	181879.360924	36.209101
1402.784904	182194.926705	36.214119
1404.248012	182499.015965	36.219136
1405.474107	182818.060073	36.224154
1407.150561	183120.619855	36.229172
1408.594849	183439.149255	36.234189
1409.612539	183756.151710	36.239207
1411.391220	184062.571204	36.244224
1412.833924	184388.189121	36.249242
1414.345546	184697.969198	36.254260
1415.911787	185010.204476	36.259277
1416.952248	185324.533942	36.264295
1418.439394	185627.265779	36.269312
1419.833982	185933.517943	36.274330
1421.117501	186258.957348	36.279348
1422.817899	186572.575475	36.284365
1424.165688	186898.566461	36.289383
1425.481032	187209.763781	36.294400
1426.578575	187529.021272	36.299418
1428.215601	187845.728778	36.304436
1429.708102	188164.239060	36.309453
1430.977709	188475.856995	36.314471
1432.566543	188767.405286	36.319488
1433.809160	189082.623349	36.324506
1435.223066	189390.706042	36.329524
1436.427432	189679.885112	36.334541
1437.169971	189996.802872	36.339559
1439.036795	190297.071893	36.344576
1440.595254	190614.886361	36.349594
1441.747600	190926.130377	36.354612
1443.441507	191231.434298	36.359629
1444.322191	191563.723364	36.364647
1445.685169	191869.516798	36.369664
1447.272037	192200.829400	36.374682
1448.504377	192532.227762	36.379700
1450.369551	192855.677860	36.384717
1451.653936	193193.748701	36.389735
1453.254490	193511.380843	36.394752
1454.768771	193845.291322	36.399770
1455.863733	194197.122321	36.404788
1457.527717	194520.449218	36.409805
1458.987832	194857.801710	36.414823
1460.766654	195197.464663	36.419840
1462.167963	195532.608723	36.424858
1463.319085	195865.523359	36.429876
1465.007478	196201.842211	36.434893
1466.493291	196550.904635	36.439911
1467.814408	196886.652906	36.444928
1469.395748	197237.417104	36.449946
1471.130230	197586.659736	36.454964
1472.400238	197925.671841	36.459981
1473.833049	198280.757281	36.464999
1475.370331	198613.685384	36.470016
1477.016156	198971.672035	36.475034
1478.336284	199314.059967	36.480052
1480.195626	199660.689928	36.485069
1481.380822	200012.803562	36.490087
1483.087949	200365.048573	36.495104
1484.615653	200714.252462	36.500122
1485.691368	201078.260719	36.505140
1487.199112	201414.013058	36.510157
1488.764368	201781.003895	36.515175
1490.047190	202135.587810	36.520192
1491.608837	202495.955208	36.525210
1492.901343	202864.774161	36.530228
1494.923653	203219.901410	36.535245
1496.147425	203580.304579	36.540263
1497.258385	203941.794688	36.545280
1499.167105	204310.620612	36.550298
1500.338349	204681.842987	36.555316
1502.088384	205037.899974	36.560333
1503.535183	205408.293144	36.565351
1505.127892	205783.666737	36.570368
1506.795465	206146.916483	36.575386
1508.357645	206523.492255	36.580404
1509.783483	206877.579697	36.585421
1511.554540	207252.143638	36.590439
1513.298828	207612.619412	36.595456
1514.920206	207968.609445	36.600474
1516.237134	208334.263533	36.605492
1518.164866	208698.942200	36.610509
1519.571039	209061.308776	36.615527
1521.077401	209412.346566	36.620544
1522.422763	209767.056753	36.625562
1523.776918	210138.020439	36.630580
1525.406563	210505.156218	36.635597
1527.128966	210874.767091	36.640615
1528.482465	211232.199477	36.645632
1530.327951	211585.514024	36.650650
1531.890738	211941.594148	36.655668
1533.475047	212272.732661	36.660685
1534.693882	212625.596221	36.665703
1535.845401	212962.726264	36.670720
1537.758398	213306.792113	36.675738
1538.778571	213651.514729	36.680756
1540.134506	213989.148175	36.685773
1541.728876	214348.940644	36.690791
1543.354532	214699.078365	36.695808
1545.007871	215061.149617	36.700826
1546.188902	215422.309798	36.705844
1547.874917	215783.464119	36.710861
1549.149697	216144.662353	36.715879
1550.609668	216507.406011	36.720896
1552.256824	216878.856977	36.725914
1553.272198	217263.925469	36.730932
1554.967319	217628.386893	36.735949
1556.837629	218010.015279	36.740967
1558.078393	218393.806385	36.745984
1559.870806	218781.393754	36.751002
1561.443188	219165.437754	36.756020
1563.333237	219536.655216	36.761037
1564.828186	219931.560027	36.766055
1566.322792	220306.477551	36.771072
1567.998992	220690.357581	36.776090
1568.943688	221077.306110	36.781108
1570.955625	221462.936737	36.786125
1572.263260	221859.200309	36.791143
1573.703473	222256.281563	36.796160
1575.564174	222655.910879	36.801178
1577.486749	223062.567008	36.806196
1578.684260	223452.961705	36.811213
1580.559414	223861.203247	36.816231
1581.884959	224251.350862	36.821248
1583.484298	224727.864422	36.826266
1584.885773	225142.132152	36.831284
1586.734108	225552.923875	36.836301
1588.170321	225948.824451	36.841319
1589.721121	226365.103611	36.846336
1591.846450	226770.544955	36.851354
1593.106316	227193.783729	36.856372
1595.107447	227595.615947	36.861389
1596.495958	227994.654955	36.866407
1597.661016	228405.263886	36.871424
1599.602695	228814.120127	36.876442
1601.248773	229228.131947	36.881460
1603.072096	229637.086380	36.886477
1604.855461	230041.527263	36.891495
1606.200865	230462.907804	36.896512
1608.112532	230865.983560	36.901530
1609.648167	231287.589061	36.906548
1611.119867	231695.311932	36.911565
1613.041893	232109.006971	36.916583
1614.598748	232528.681927	36.921600
1616.198805	232926.277173	36.926618
1617.740025	233341.714862	36.931636
1619.587922	233751.489248	36.936653
1621.002352	234152.064735	36.941671
1622.693056	234571.621274	36.946688
1624.507042	234981.175664	36.951706
1626.005480	235402.874331	36.956724
1628.078135	235803.903775	36.961741
1629.504805	236221.780586	36.966759
1630.746711	236629.477349	36.971776
1632.466113	237039.356890	36.976794
1633.989520	237456.356831	36.981812
1635.779496	237873.364440	36.986829
1637.307662	238286.631279	36.991847
1638.887425	238696.511968	36.996864
1640.576433	239094.131603	37.001882
1641.767928	239493.866354	37.006900
1643.230572	239887.257309	37.011917
1645.145126	240284.486269	37.016935
1646.720988	240698.003964	37.021952
1648.120368	241100.272914	37.026970
1649.348222	241514.865654	37.031988
1651.109062	241927.491287	37.037005
1652.512082	242346.552747	37.042023
1654.059774	242765.540202	37.047040
1655.766690	243192.072001	37.052058
1657.125754	243629.153226	37.057076
1658.833566	244053.603229	37.062093
1660.484205	244494.524259	37.067111
1661.800857	244932.656027	37.072128
1663.623912	245370.755589	37.077146
1665.323617	245823.228731	37.082164
1666.669722	246272.433152	37.087181
1668.397105	246720.762307	37.092199
1670.306456	247172.389767	37.097216
1672.322219	247626.616723	37.102234
1673.758177	248092.472954	37.107252
1675.469377	248543.042481	37.112269
1677.016884	248997.170567	37.117287
1678.659064	249471.961579	37.122304
1680.372619	249916.181408	37.127322
1681.658949	250394.791810	37.132340
1683.792145	250855.556808	37.137357
1685.829482	251325.711802	37.142375
1687.089566	251809.205224	37.147392
1689.150930	252272.828403	37.152410
1690.827587	252739.004975	37.157428
1692.235619	253214.701631	37.162445
1694.454824	253685.895237	37.167463
1695.709039	254166.698517	37.172480
1697.798606	254621.503546	37.177498
1699.555737	255113.681090	37.182516
1701.390628	255575.158835	37.187533
1703.377146	256044.537518	37.192551
1705.098155	256524.197722	37.197568
1706.947440	256977.392021	37.202586
1708.591827	257458.792508	37.207604
1710.391233	257936.128329	37.212621
1712.364632	258399.870081	37.217639
1713.663147	258868.168897	37.222656
1715.755921	259327.546963	37.227674
1717.394302	259803.842434	37.232692
1719.152200	260288.907637	37.237709
1720.883694	260759.446422	37.242727
1722.085395	261228.954854	37.247744
1724.150250	261709.599626	37.252762
1725.738606	262186.791874	37.257780
1727.767693	262667.721613	37.262797
1729.668799	263132.185557	37.267815
1730.902060	263613.906749	37.272832
1732.951155	264073.925576	37.277850
1734.877045	264555.430170	37.282868
1736.516269	265042.341845	37.287885
1738.214336	265512.705971	37.292903
1739.919350	265988.301622	37.297920
1741.709610	266465.000520	37.302938
1743.647704	266948.177753	37.307956
1745.215440	267421.965742	37.312973
1747.083810	267891.461283	37.317991
1748.586573	268375.852066	37.323008
1750.624045	268850.119794	37.328026
1752.204807	269327.383730	37.333044
1754.084823	269787.857120	37.338061
1755.726428	270249.639451	37.343079
1757.813272	270707.333985	37.348096
1758.919140	271159.042440	37.353114
1760.800952	271607.624581	37.358132
1762.482204	272069.245410	37.363149
1764.156657	272526.522798	37.368167
1765.451141	273000.526374	37.373184
1767.653950	273461.118970	37.378202
1769.313768	273930.107118	37.383220
1770.562503	274398.578077	37.388237
1772.410022	274869.464137	37.393255
1774.097722	275358.995692	37.398272
1775.884744	275843.302371	37.403290
1777.615379	276328.735076	37.408308
1779.306477	276817.246962	37.413325
1781.292354	277305.607489	37.418343
1782.585774	277803.099057	37.423360
1784.292543	278294.196069	37.428378
1786.348781	278804.234924	37.433396
1787.847796	279302.552605	37.438413
1789.807379	279810.775910	37.443431
1791.346420	280318.635498	37.448448
1793.187785	280843.589976	37.453466
1795.438653	281351.151366	37.458484
1796.745287	281876.216575	37.463501
1798.969768	282387.030767	37.468519
1800.506491	282916.474695	37.473536
1802.072181	283430.899952	37.478554
1804.335662	283950.491828	37.483572
1805.992579	284487.632844	37.488589
1808.354118	285005.985827	37.493607
1809.688805	285535.302106	37.498624
1811.498393	286066.214569	37.503642
1813.623001	286594.533024	37.508660
1815.411113	287124.327581	37.513677
1817.280870	287655.402129	37.518695
1818.953533	288188.920275	37.523712
1820.845483	288717.929660	37.528730
1822.852437	289264.698254	37.533748
1824.412757	289801.251253	37.538765
1826.410675	290328.052318	37.543783
1828.537129	290878.731463	37.548800
1830.085263	291409.640953	37.553818
1831.920936	291947.409452	37.558836
1833.858429	292491.178510	37.563853
1835.848348	293028.662751	37.568871
1837.525605	293571.885679	37.573888
1839.542283	294104.991871	37.578906
1841.706204	294652.345661	37.583924
1843.356406	295196.606752	37.588941
1845.330833	295732.658560	37.593959
1846.976946	296269.346149	37.598976
1848.913282	296814.720327	37.603994
1850.918718	297366.633157	37.609012
1852.660901	297909.798689	37.614029
1854.721873	298443.917714	37.619047
1856.414661	298991.124051	37.624064
1858.430288	299542.718778	37.629082
1860.536196	300074.612131	37.634100
1862.020471	300616.129449	37.639117
1864.009403	301157.687398	37.644135
1865.971076	301700.516669	37.649152
1867.718960	302235.936700	37.654170
1869.480908	302790.907217	37.659188
1871.343837	303329.730577	37.664205
1873.362051	303870.074327	37.669223
1874.889042	304420.730859	37.674240
1876.884590	304957.033712	37.679258
1878.965879	305476.354299	37.684276
1880.642509	306013.363657	37.689293
1882.526266	306527.478919	37.694311
1884.460311	307045.925491	37.699328
1885.568904	307568.441540	37.704346
1887.931114	308099.000899	37.709364
1889.437637	308631.907557	37.714381
1891.572681	309162.599130	37.719399
1893.386773	309704.996605	37.724416
1894.966491	310254.184172	37.729434
1897.208922	310786.548688	37.734452
1898.862928	311335.665644	37.739469
1900.569460	311886.852378	37.744487
1902.547972	312443.932499	37.749504
1904.387330	313007.253059	37.754522
1906.129321	313555.171363	37.759540
1907.877999	314117.381188	37.764557
1909.930702	314686.291188	37.769575
1911.695521	315256.412371	37.774592
1913.251088	315836.009837	37.779610
1915.387615	316396.233438	37.784628
1917.026391	316989.748450	37.789645
1918.836940	317580.386101	37.794663
1920.498059	318170.916424	37.799680
1922.635437	318773.932079	37.804698
1924.514287	319368.961246	37.809716
1926.409992	319973.326465	37.814733
1928.383982	320588.972419	37.819751
1930.295891	321193.425384	37.824768
1932.179001	321804.022094	37.829786
1934.309998	322417.238115	37.834804
1936.144537	323027.094895	37.839821
1938.242854	323645.738019	37.844839
1940.095896	324260.987907	37.849856
1941.934914	324890.350661	37.854874
1943.897589	325500.644525	37.859892
1945.625618	326129.403534	37.864909
1947.829284	326767.598286	37.869927
1949.461620	327392.932391	37.874944
1951.688751	328029.865707	37.879962
1953.705700	328664.440348	37.884980
1955.652638	329293.612040	37.889997
1957.738949	329925.444935	37.895015
1959.774114	330572.080032	37.900032
1961.574359	331205.748444	37.905050
1963.989483	331848.853555	37.910068
1965.760501	332485.685622	37.915085
1967.813771	333121.778318	37.920103
1969.489018	333766.937976	37.925120
1971.614723	334406.405407	37.930138
1974.081806	335044.539616	37.935156
1975.909305	335679.649462	37.940173
1977.849522	336316.053070	37.945191
1979.947338	336967.577312	37.950208
1981.980930	337611.285765	37.955226
1984.386403	338248.934266	37.960244
1985.960993	338883.209122	37.965261
1987.804913	339533.143630	37.970279
1990.172454	340164.504761	37.975296
1992.152530	340811.100501	37.980314
1994.179984	341443.796060	37.985332
1995.955236	342090.028154	37.990349
1997.738511	342722.772906	37.995367
1999.879405	343366.998692	38.000384
2002.052962	344011.438883	38.005402
2004.492856	344653.999019	38.010420
2006.200711	345307.381633	38.015437
2008.521939	345932.254151	38.020455
2010.145664	346543.376395	38.025472
2012.077917	347153.957445	38.030490
2014.133950	347758.672888	38.035508
2015.996519	348384.247808	38.040525
2017.788900	348997.415911	38.045543
2019.868194	349613.294459	38.050560
2021.838307	350251.083076	38.055578
2023.727162	350859.108948	38.060596
2025.700444	351503.400867	38.065613
2027.826479	352123.322431	38.070631
2029.728664	352752.635781	38.075648
2031.557558	353401.262729	38.080666
2034.004036	354035.161945	38.085684
2035.523091	354680.039817	38.090701
2037.775133	355329.760217	38.095719
2039.854180	355974.094534	38.100736
2041.536481	356632.363691	38.105754
2044.245073	357283.297799	38.110772
2045.999615	357943.995370	38.115789
2047.369029	358607.004008	38.120807
2049.686388	359262.690516	38.125824
2051.650182	359942.426084	38.130842
2053.624607	360603.196317	38.135860
2055.646817	361289.495834	38.140877
2057.532466	361964.795415	38.145895
2059.441565	362649.314100	38.150912
2061.677643	363343.990615	38.155930
2063.983244	364029.662714	38.160948
2065.944595	364722.076700	38.165965
2067.940081	365421.245765	38.170983
2070.159154	366123.713587	38.176000
2071.940041	366832.582437	38.181018
2073.812767	367513.392907	38.186036
2076.156169	368232.796318	38.191053
2078.291704	368951.002571	38.196071
2080.788013	369652.166146	38.201088
2082.321903	370376.835846	38.206106
2084.675763	371079.339869	38.211124
2086.656927	371805.023245	38.216141
2088.847969	372529.313097	38.221159
2091.028628	373239.691379	38.226176
2092.631848	373969.856974	38.231194
2095.011688	374687.528267	38.236212
2097.400545	375421.870822	38.241229
2099.302875	376145.424001	38.246247
2101.701127	376864.847988	38.251264
2103.978635	377605.680074	38.256282
2106.386172	378324.564729	38.261300
2108.179569	379057.583984	38.266317
2109.984307	379776.689493	38.271335
2112.366678	380504.736723	38.276352
2114.726097	381242.762325	38.281370
2116.717247	381970.918128	38.286388
2118.982001	382697.820985	38.291405
2121.056519	383419.972421	38.296423
2123.248903	384149.998928	38.301440
2125.262852	384888.785463	38.306458
2127.432520	385614.751386	38.311476
2129.790770	386349.644515	38.316493
2131.755520	387079.413841	38.321511
2134.098742	387807.405330	38.326528
2135.954961	388544.282436	38.331546
2138.450330	389277.056712	38.336564
2140.225880	390019.590735	38.341581
2142.551750	390752.713034	38.346599
2145.084460	391483.122144	38.351616
2146.667441	392213.011546	38.356634
2148.864169	392937.940828	38.361652
2150.787415	393650.554124	38.366669
2153.280651	394356.314442	38.371687
2155.518364	395059.692493	38.376704
2157.280146	395774.132114	38.381722
2159.115356	396473.690727	38.386740
2161.197165	397199.777394	38.391757
2163.333670	397917.093757	38.396775
2165.405580	398634.301773	38.401792
2167.755789	399362.900546	38.406810
2169.741782	400084.014771	38.411828
2171.942505	400808.749797	38.416845
2173.962065	401545.811439	38.421863
2176.191413	402276.307205	38.426880
2177.932408	403027.059398	38.431898
2180.409450	403759.604277	38.436916
2182.419784	404506.978508	38.441933
2184.429432	405261.984366	38.446951
2186.974991	406018.350651	38.451968
2188.816653	406787.150472	38.456986
2191.122055	407548.758598	38.462004
2193.051217	408313.903575	38.467021
2195.290227	409093.111529	38.472039
2197.393367	409860.489329	38.477056
2199.402076	410652.102866	38.482074
2201.628845	411418.047720	38.487092
2204.048561	412212.460054	38.492109
2205.952163	413007.921526	38.497127
2208.561198	413801.722795	38.502144
2210.881808	414600.207837	38.507162
2213.025691	415397.051300	38.512180
2215.149433	416198.457555	38.517197
2217.308847	416999.832979	38.522215
2219.621890	417799.207999	38.527232
2221.564808	418617.713013	38.532250
2223.911764	419424.476450	38.537268
2226.210355	420237.856415	38.542285
2228.547591	421060.850985	38.547303
2231.023904	421864.172246	38.552320
2233.000476	422690.540084	38.557338
2235.436526	423509.917795	38.562356
2237.870686	424323.344155	38.567373
2240.005767	425151.932351	38.572391
2242.299649	425979.605390	38.577408
2244.620525	426803.448414	38.582426
2246.664513	427630.701092	38.587444
2248.942699	428453.178282	38.592461
2251.066257	429293.624564	38.597479
2253.165002	430111.770926	38.602496
2255.083412	430959.431100	38.607514
2257.931730	431795.416563	38.612532
2260.364761	432648.954483	38.617549
2262.535571	433492.128094	38.622567
2265.134470	434330.037714	38.627584
2267.267418	435166.222341	38.632602
2269.348576	436004.409459	38.637620
2271.780245	436844.835955	38.642637
2274.003572	437685.113928	38.647655
2276.645908	438523.672166	38.652672
2278.628104	439368.684081	38.657690
2281.053564	440213.135554	38.662708
2283.559274	441052.684272	38.667725
2285.520617	441903.928424	38.672743
2287.993647	442742.052331	38.677760
2290.207269	443592.228306	38.682778
2292.284046	444434.501571	38.687796
2294.660313	445281.397650	38.692813
2296.486011	446137.760761	38.697831
2299.184896	446976.544394	38.702848
2301.614233	447806.841722	38.707866
2303.625494	448617.094927	38.712884
2305.870714	449432.033167	38.717901
2307.835257	450260.237739	38.722919
2310.397286	451080.016794	38.727936
2312.581472	451918.184456	38.732954
2314.791687	452750.599641	38.737972
2317.142236	453573.501873	38.742989
2319.080266	454413.784210	38.748007
2321.603217	455251.407543	38.753024
2323.773343	456101.240754	38.758042
2325.757036	456948.086320	38.763060
2328.731043	457797.311784	38.768077
2330.749632	458652.928435	38.773095
2332.756621	459505.477459	38.778112
2334.954419	460376.258961	38.783130
2337.254189	461238.038310	38.788148
2339.781198	462118.091958	38.793165
2342.222485	463003.276424	38.798183
2344.947446	463884.634173	38.803200
2347.100576	464761.498050	38.808218
2349.262054	465650.753954	38.813236
2351.639881	466529.775671	38.818253
2353.790748	467435.073062	38.823271
2356.356785	468327.980200	38.828288
2358.532456	469224.851656	38.833306
2360.636740	470139.225964	38.838324
2363.284310	471040.128165	38.843341
2365.618756	471966.452206	38.848359
2368.109125	472878.155320	38.853376
2370.541700	473803.918262	38.858394
2372.502752	474724.661759	38.863412
2375.434338	475646.361470	38.868429
2377.841846	476566.334066	38.873447
2379.936872	477489.999533	38.878464
2382.597774	478422.515221	38.883482
2384.587460	479355.902283	38.888500
2387.472846	480278.236333	38.893517
2389.966090	481229.523298	38.898535
2392.025406	482160.230016	38.903552
2394.713257	483090.482008	38.908570
2396.559348	484034.709283	38.913588
2399.739799	484981.342291	38.918605
2402.100845	485927.151411	38.923623
2404.203726	486865.128011	38.928640
2407.134491	487810.540423	38.933658
2409.307154	488749.364198	38.938676
2411.785633	489690.863156	38.943693
2413.999952	490640.631980	38.948711
2416.722845	491587.590088	38.953728
2419.301601	492535.680749	38.958746
2421.480602	493483.684181	38.963764
2423.819551	494431.507835	38.968781
2426.436720	495385.691359	38.973799
2428.589268	496344.691048	38.978816
2431.398735	497292.580133	38.983834
2433.544449	498250.261869	38.988852
2436.198538	499194.285750	38.993869
2438.490188	500159.602745	38.998887
2440.982108	501120.392033	39.003904
2443.668271	502080.135270	39.008922
2445.727974	503033.369698	39.013940
2448.323488	503991.301779	39.018957
2450.853556	504957.055307	39.023975
2453.699130	505915.236729	39.028992
2455.821265	506873.985184	39.034010
2458.349782	507834.071902	39.039028
2460.806082	508773.392474	39.044045
2463.396517	509707.947541	39.049063
2466.055329	510635.429719	39.054080
2468.520334	511554.673520	39.059098
2470.861563	512481.898706	39.064116
2473.133215	513391.944619	39.069133
2475.422200	514318.516053	39.074151
2477.281369	515252.763724	39.079168
2480.124918	516187.901763	39.084186
2482.332754	517126.766903	39.089204
2484.933508	518072.917119	39.094221
2487.108216	519029.257014	39.099239
2489.382210	519977.006942	39.104256
2492.105321	520943.062015	39.109274
2494.020821	521908.584747	39.114292
2496.623590	522879.574289	39.119309
2499.106113	523857.220263	39.124327
2501.239799	524844.228119	39.129344
2504.079766	525833.371265	39.134362
2506.390008	526831.097176	39.139380
2509.067149	527823.509452	39.144397
2511.357821	528818.336053	39.149415
2513.552752	529823.936190	39.154432
2516.391243	530834.849040	39.159450
2518.894938	531862.460395	39.164468
2521.165725	532876.698939	39.169485
2523.362391	533910.710272	39.174503
2526.004961	534940.044825	39.179520
2528.944012	535964.325336	39.184538
2531.499556	537009.781852	39.189556
2533.859557	538045.935945	39.194573
2536.099557	539089.129129	39.199591
2539.041661	540139.425178	39.204608
2541.687718	541181.643178	39.209626
2544.385668	542254.611755	39.214644
2546.980408	543304.327501	39.219661
2549.717785	544353.035827	39.224679
2552.181713	545407.795878	39.229696
2555.046945	546461.152588	39.234714
2557.538751	547530.028730	39.239732
2560.550123	548587.875861	39.244749
2562.952607	549649.764218	39.249767
2565.238340	550710.986290	39.254784
2567.952383	551765.067866	39.259802
2570.493501	552844.982669	39.264820
2573.276042	553906.225332	39.269837
2575.737438	554986.133081	39.274855
2578.129253	556050.085694	39.279872
2580.812420	557106.368417	39.284890
2583.258609	558195.466741	39.289908
2586.124960	559269.937230	39.294925
2588.656036	560354.322700	39.299943
2591.112100	561426.927263	39.304960
2593.738922	562507.151312	39.309978
2596.588426	563602.015432	39.314996
2598.994626	564673.809829	39.320013
2601.889826	565755.829872	39.325031
2604.669815	566843.251572	39.330048
2607.131129	567925.412619	39.335066
2609.898943	569012.351915	39.340084
2612.353991	570090.566143	39.345101
2614.852640	571176.663022	39.350119
2617.609110	572265.184296	39.355136
2620.285897	573349.961588	39.360154
2622.756835	574441.203211	39.365172
2625.254165	575531.091350	39.370189
2627.920794	576620.505544	39.375207
2630.344628	577713.376509	39.380224
2632.849598	578787.075687	39.385242
2635.788209	579858.654084	39.390260
2638.392729	580905.467913	39.395277
2640.911571	581965.045566	39.400295
2643.103638	583027.293515	39.405312
2645.876643	584084.940778	39.410330
2648.281414	585148.122273	39.415348
2650.941345	586221.245445	39.420365
2653.628394	587297.276689	39.425383
2655.922062	588371.221639	39.430400
2658.763533	589454.553198	39.435418
2660.979435	590554.929230	39.440436
2663.810771	591641.321698	39.445453
2666.445075	592742.128139	39.450471
2668.924322	593843.158457	39.455488
2671.438277	594947.587143	39.460506
2673.939191	596073.153431	39.465524
2676.649341	597203.285337	39.470541
2679.371417	598324.841943	39.475559
2681.729620	599460.272094	39.480576
2684.212038	600602.530710	39.485594
2687.059387	601765.644698	39.490612
2689.370416	602898.892223	39.495629
2692.223987	604067.028844	39.500647
2694.745211	605237.703635	39.505664
2697.623045	606403.795108	39.510682
2699.739049	607597.365599	39.515700
2702.667510	608769.110192	39.520717
2705.835431	609961.306489	39.525735
2708.333668	611156.238057	39.530752
2711.245447	612354.225127	39.535770
2713.489863	613554.944332	39.540788
2716.296243	614755.591054	39.545805
2719.341602	615962.368653	39.550823
2721.937608	617182.088031	39.555840
2724.805604	618387.428902	39.560858
2727.508458	619602.361942	39.565876
2730.225635	620813.358573	39.570893
2733.391080	622049.634517	39.575911
2735.820302	623269.150328	39.580928
2738.723595	624489.449385	39.585946
2741.427556	625725.729813	39.590964
2744.152073	626963.712416	39.595981
2747.077414	628197.122803	39.600999
2749.767427	629439.268694	39.606016
2752.326693	630665.760210	39.611034
2754.956043	631910.022782	39.616052
2757.776489	633154.256398	39.621069
2761.276679	634393.088521	39.626087
2763.928618	635644.940789	39.631104
2767.059613	636876.550747	39.636122
2769.745252	638133.487405	39.641140
2772.587546	639361.206456	39.646157
2775.243304	640612.207744	39.651175
2777.768852	641849.459914	39.656192
2780.783594	643091.219938	39.661210
2783.572042	644348.226037	39.666228
2786.092954	645587.269079	39.671245
2789.286844	646843.499772	39.676263
2791.886044	648089.153128	39.681280
2794.956547	649337.465324	39.686298
2797.753934	650591.498083	39.691316
2800.389927	651839.270253	39.696333
2803.671994	653090.765396	39.701351
2806.237335	654347.501576	39.706368
2809.247895	655584.526834	39.711386
2812.023513	656830.052078	39.716404
2814.913294	658083.069723	39.721421
2817.769181	659309.042625	39.726439
2820.443677	660523.987179	39.731456
2823.530654	661721.685737	39.736474
2825.876649	662932.349961	39.741492
2828.519910	664136.342934	39.746509
2831.354155	665339.805198	39.751527
2834.023811	666556.229792	39.756544
2836.532432	667771.132883	39.761562
2839.485139	668990.881667	39.766580
2841.988753	670221.340992	39.771597
2844.741773	671448.266948	39.776615
2847.072079	672697.976796	39.781632
2850.193520	673942.815709	39.786650
2853.093853	675197.169760	39.791668
2855.462918	676454.126861	39.796685
2858.653953	677729.167204	39.801703
2860.985110	678998.310177	39.806720
2863.896430	680276.176161	39.811738
2866.605485	681560.604679	39.816756
2869.531238	682855.596343	39.821773
2872.391234	684143.561718	39.826791
2875.053193	685452.432415	39.831808
2877.718222	686756.099292	39.836826
2880.696210	688086.284326	39.841844
2883.427423	689410.605772	39.846861
2886.296912	690735.503351	39.851879
2889.271772	692079.688584	39.856896
2892.009823	693410.513303	39.861914
2895.250914	694760.501512	39.866932
2897.709150	696109.619649	39.871949
2900.828219	697455.496988	39.876967
2903.492181	698830.348878	39.881984
2906.609060	700199.903584	39.887002
2909.413110	701576.135653	39.892020
2912.666390	702946.525624	39.897037
2915.186476	704319.545548	39.902055
2917.900774	705706.138352	39.907072
2920.650231	707097.505536	39.912090
2923.562485	708494.068669	39.917108
2926.459493	709903.133106	39.922125
2929.605281	711306.279572	39.927143
2932.352789	712718.566783	39.932160
2935.323951	714138.500950	39.937178
2938.221449	715551.824744	39.942196
2940.855422	716975.097663	39.947213
2944.135544	718401.930617	39.952231
2946.781677	719845.144519	39.957248
2949.910583	721276.011720	39.962266
2953.034643	722709.154633	39.967284
2955.957255	724152.167216	39.972301
2958.675939	725598.074615	39.977319
2961.715219	727042.488533	39.982336
2964.706442	728488.236502	39.987354
2967.869241	729939.282111	39.992372
2970.999719	731395.753964	39.997389
2973.895984	732833.928328	40.002407
2976.699373	734286.772646	40.007424
2979.821918	735746.212975	40.012442
2982.939680	737192.407645	40.017460
2986.012034	738645.009756	40.022477
2989.085244	740110.569178	40.027495
2991.684460	741557.980183	40.032512
2994.852272	743019.285849	40.037530
2997.858866	744485.130103	40.042548
3000.769477	745937.207828	40.047565
3004.146663	747407.768748	40.052583
3007.270492	748872.081485	40.057600
3010.086432	750326.018591	40.062618
3013.172439	751757.419849	40.067636
3015.892408	753184.182933	40.072653
3018.859450	754600.840594	40.077671
3021.798642	756012.711212	40.082688
3024.640312	757426.109234	40.087706
3028.264688	758840.740149	40.092724
3031.059863	760269.760988	40.097741
3034.090552	761681.056129	40.102759
3036.736217	763107.301555	40.107776
3039.558090	764535.017889	40.112794
3043.019980	765955.128304	40.117812
3045.820281	767407.967817	40.122829
3048.775077	768830.711303	40.127847
3051.744249	770290.922194	40.132864
3054.926894	771746.878828	40.137882
3057.864435	773194.335336	40.142900
3060.534428	774665.813455	40.147917
3063.034005	776150.920621	40.152935
3066.226575	777627.412546	40.157952
3069.502025	779102.756638	40.162970
3072.503773	780605.425558	40.167988
3074.984977	782109.045317	40.173005
3078.263100	783610.453835	40.178023
3081.332535	785141.891677	40.183040
3083.936168	786658.564588	40.188058
3087.238390	788196.810879	40.193076
3090.176562	789740.469486	40.198093
3093.523463	791282.793145	40.203111
3096.302207	792839.129547	40.208128
3099.651678	794401.394779	40.213146
3102.649220	795953.429091	40.218164
3105.415514	797529.145890	40.223181
3108.685265	799099.332547	40.228199
3111.775624	800686.956849	40.233216
3114.803210	802273.444057	40.238234
3118.037067	803860.069916	40.243252
3120.892482	805470.059695	40.248269
3124.149938	807064.106229	40.253287
3127.562388	808677.990110	40.258304
3130.375957	810284.308138	40.263322
3133.796406	811890.584715	40.268340
3137.075306	813510.569063	40.273357
3140.285661	815134.422693	40.278375
3143.361477	816749.312636	40.283392
3146.468805	818369.907777	40.288410
3149.450438	820003.889361	40.293428
3152.520120	821634.965792	40.298445
3156.158640	823260.717417	40.303463
3159.426287	824900.366569	40.308480
3161.932303	826531.395704	40.313498
3165.459140	828167.161968	40.318516
3168.669971	829814.945328	40.323533
3172.109512	831459.398951	40.328551
3175.223946	833104.267439	40.333568
3178.227570	834741.237052	40.338586
3181.687818	836384.674776	40.343604
3185.109677	838045.458307	40.348621
3188.639837	839676.943474	40.353639
3191.904124	841334.171344	40.358656
3195.190219	842976.715856	40.363674
3198.569617	844597.721011	40.368692
3201.911728	846249.028774	40.373709
3205.024728	847885.947248	40.378727
3208.256788	849524.749092	40.383744
3211.468593	851170.310142	40.388762
3214.924714	852813.064728	40.393780
3217.794000	854453.538711	40.398797
3221.168228	856084.371388	40.403815
3224.906635	857704.524813	40.408832
3228.019311	859306.797721	40.413850
3231.476742	860887.164186	40.418868
3234.058078	862469.785249	40.423885
3237.296648	864063.224373	40.428903
3240.426049	865655.971086	40.433920
3243.614850	867248.965333	40.438938
3246.892209	868844.234224	40.443956
3249.795803	870443.109196	40.448973
3252.889998	872051.009698	40.453991
3256.106119	873662.035864	40.459008
3258.726760	875283.943746	40.464026
3262.038736	876908.774337	40.469044
3265.345742	878558.197839	40.474061
3268.459093	880199.554616	40.479079
3271.387037	881848.308497	40.484096
3274.838055	883515.540143	40.489114
3278.042194	885184.072835	40.494132
3281.371329	886873.247341	40.499149
3284.437339	888546.336206	40.504167
3287.848528	890233.837339	40.509184
3290.919741	891932.183755	40.514202
3294.274095	893643.286315	40.519220
3297.810130	895351.338970	40.524237
3300.942217	897072.436415	40.529255
3304.746847	898787.504851	40.534272
3307.810568	900504.100297	40.539290
3311.085536	902228.513490	40.544308
3314.702682	903961.579926	40.549325
3317.887787	905696.489150	40.554343
3321.408264	907421.087092	40.559360
3324.736629	909170.663407	40.564378
3327.970027	910908.358307	40.569396
3331.508735	912663.425739	40.574413
3335.089817	914403.610869	40.579431
3338.731483	916159.271227	40.584448
3341.815131	917921.658990	40.589466
3345.631511	919664.255218	40.594484
3349.196759	921413.144408	40.599501
3352.511861	923170.716108	40.604519
3356.197141	924922.666768	40.609536
3359.506574	926674.490354	40.614554
3362.857569	928428.607484	40.619572
3366.322155	930190.174484	40.624589
3369.710733	931948.871241	40.629607
3373.155687	933688.403312	40.634624
3376.550681	935453.972561	40.639642
3379.972876	937207.464741	40.644660
3383.346646	938962.194751	40.649677
3386.803237	940731.616741	40.654695
3390.417886	942479.577742	40.659712
3393.897483	944247.033442	40.664730
3397.198744	946009.998471	40.669748
3400.534548	947769.299358	40.674765
3404.361400	949532.497143	40.679783
3407.817240	951283.509326	40.684800
3411.245884	953068.721595	40.689818
3415.188049	954862.274226	40.694836
3418.543543	956663.874499	40.699853
3421.739084	958456.530783	40.704871
3425.476394	960249.615413	40.709888
3428.557609	962056.514614	40.714906
3431.912993	963850.103887	40.719924
3435.572021	965646.989386	40.724941
3438.756903	967448.076378	40.729959
3442.618493	969256.000582	40.734976
3445.789323	971060.444646	40.739994
3449.243879	972858.325168	40.745012
3452.682632	974638.666474	40.750016
3455.890398	976372.152487	40.755021
3459.366417	978040.990562	40.760026
3462.309492	979677.691871	40.765031
3465.859115	981217.662894	40.770036
3469.260107	982701.415157	40.775040
3472.231073	984085.226548	40.780045
3475.511944	985396.167982	40.785050
3478.371777	986642.505178	40.790055
3481.262919	987794.464289	40.795060
3484.034037	988882.058433	40.800064
3486.535766	989891.799633	40.805069
3489.431058	990820.501298	40.810074
3491.479242	991674.059378	40.815079
3493.838518	992453.583579	40.820084
3495.899581	993174.694716	40.825088
3498.107896	993837.731287	40.830093
3500.187617	994423.181728	40.835098
3501.945459	994953.696593	40.840103
3503.391490	995418.577552	40.845108
3505.218624	995831.748717	40.850112
3506.779937	996202.383303	40.855117
3508.423269	996502.683662	40.860122
3509.617882	996762.443178	40.865127
3511.185289	996983.089797	40.870132
3512.423255	997164.451714	40.875136
3513.862132	997293.984493	40.880141
3514.928256	997381.229057	40.885146
3515.734870	997421.885389	40.890151
3516.701183	997427.080489	40.895156
3517.791764	997411.617278	40.900160
3518.389848	997366.349025	40.905165
3519.958061	997290.839363	40.910170
3520.433858	997183.187770	40.915175
3521.114635	997041.718351	40.920180
3521.971660	996884.152404	40.925184
3522.745405	996690.377687	40.930189
3523.239634	996481.940390	40.935194
3523.537845	996246.361988	40.940199
3524.478489	995991.193427	40.945204
3524.679645	995723.281405	40.950208
3525.228834	995445.950702	40.955213
3525.778930	995141.435261	40.960218
3526.476571	994828.698177	40.965223
3527.054340	994478.659979	40.970228
3526.943130	994134.752783	40.975232
3527.265608	993780.719984	40.980237
3527.817045	993394.771969	40.985242
3527.908223	993017.057150	40.990247
3528.377261	992625.906963	40.995252
3528.575115	992217.917820	41.000256
3528.667501	991810.598847	41.005261
3529.231922	991379.492104	41.010266
3529.298534	990956.328863	41.015271
3529.952398	990507.988402	41.020276
3529.757927	990050.394754	41.025280
3529.826914	989604.028829	41.030285
3530.241887	989136.317966	41.035290
3529.905199	988671.032425	41.040295
3530.634775	988191.297189	41.045300
3531.068717	987716.738496	41.050304
3531.039332	987234.804803	41.055309
3530.914146	986733.339770	41.060314
3531.017294	986246.326414	41.065319
3530.992562	985743.294506	41.070324
3530.820078	985240.632725	41.075328
3530.762972	984745.810395	41.080333
3531.377269	984231.612324	41.085338
3531.291703	983727.631819	41.090343
3530.802202	983202.105460	41.095348
3531.157958	982683.613873	41.100352
3531.017196	982168.182848	41.105357
3531.038309	981651.897620	41.110362
3530.974460	981145.732917	41.115367
3531.390422	980617.378485	41.120372
3530.845970	980099.972001	41.125376
3531.172404	979571.340215	41.130381
3531.101104	979036.279236	41.135386
3531.284444	978519.586267	41.140391
3531.210021	977985.990180	41.145396
3531.338081	977458.953857	41.150400
3531.261284	976923.402832	41.155405
3531.655262	976381.959265	41.160410
3531.064222	975850.203074	41.165415
3531.264554	975311.035260	41.170420
3531.149524	974774.605208	41.175424
3531.059026	974236.947881	41.180429
3531.219541	973711.711275	41.185434
3530.857014	973171.261549	41.190439
3530.949858	972636.161069	41.195444
3531.271002	972087.772425	41.200448
3531.157978	971545.368105	41.205453
3530.939620	971007.037426	41.210458
3530.491020	970464.683915	41.215463
3530.644131	969922.571241	41.220468
3530.869920	969385.678084	41.225472
3530.726160	968838.229122	41.230477
3530.708401	968304.405716	41.235482
3530.575458	967763.114595	41.240487
3530.392294	967216.887451	41.245492
3530.467767	966687.204375	41.250496
3530.097957	966149.323615	41.255501
3530.241455	965598.581880	41.260506
3530.175148	965076.898793	41.265511
3530.312855	964534.279770	41.270516
3530.459612	963992.978931	41.275520
3530.055167	963454.655833	41.280525
3530.308528	962910.297669	41.285530
3529.767468	962376.401342	41.290535
3529.796763	961841.871727	41.295540
3530.013413	961299.228414	41.300544
3529.545482	960770.853129	41.305549
3529.880490	960233.478521	41.310554
3529.347196	959706.780099	41.315559
3529.157137	959165.472662	41.320564
3529.250879	958645.042037	41.325568
3528.848743	958120.235228	41.330573
3529.310075	957595.336425	41.335578
3528.927760	957065.332844	41.340583
3528.803187	956552.886521	41.345588
3528.825037	956027.035026	41.350592
3528.584680	955503.140111	41.355597
3528.797063	954974.807835	41.360602
3528.518746	954461.710820	41.365607
3528.449005	953936.762942	41.370612
3528.467883	953420.974157	41.375616
3528.424681	952908.092820	41.380621
3528.466192	952384.477164	41.385626
3528.278908	951893.549741	41.390631
3527.900411	951382.617140	41.395636
3528.016257	950881.308440	41.400640
3527.879361	950391.471540	41.405645
3527.737103	949892.117129	41.410650
3527.631939	949394.717116	41.415655
3526.968321	948892.384897	41.420660
3527.331044	948403.519256	41.425664
3527.343407	947906.433848	41.430669
3527.120035	947414.986447	41.435674
3526.934529	946945.885704	41.440679
3526.965504	946452.294091	41.445684
3526.861787	945966.432609	41.450688
3526.706301	945483.214914	41.455693
3526.735414	944994.080022	41.460698
3526.612878	944531.835415	41.465703
3526.537739	944040.903521	41.470708
3526.859191	943561.641701	41.475712
3526.607006	943077.927517	41.480717
3526.663234	942591.817981	41.485722
3526.323238	942112.435235	41.490727
3526.168888	941630.773645	41.495732
3526.188873	941156.130324	41.500736
3525.855288	940685.335592	41.505741
3526.113614	940192.930172	41.510746
3525.669613	939736.541284	41.515751
3525.779269	939261.614577	41.520756
3525.496211	938790.065026	41.525760
3525.259262	938332.943963	41.530765
3525.330626	937862.786482	41.535770
3525.239422	937410.259535	41.540775
3524.834692	936947.962264	41.545780
3525.253523	936488.749767	41.550784
3524.642675	936039.834995	41.555789
3524.803306	935575.884728	41.560794
3524.752603	935127.663115	41.565799
3524.583479	934667.428803	41.570804
3524.624391	934210.094417	41.575808
3524.426492	933768.306598	41.580813
3524.433654	933314.738820	41.585818
3524.044574	932870.891816	41.590823
3524.234870	932427.008047	41.595828
3524.148527	931976.604517	41.600832
3523.754477	931535.718241	41.605837
3523.714730	931097.041287	41.610842
3523.569345	930653.448149	41.615847
3523.491624	930226.900625	41.620852
3523.781702	929780.473855	41.625856
3523.150598	929348.568662	41.630861
3523.459057	928916.761753	41.635866
3523.157794	928489.823476	41.640871
3523.270466	928058.363471	41.645876
3522.938238	927637.510600	41.650880
3522.707698	927212.860373	41.655885
3522.711495	926785.639297	41.660890
3522.634567	926365.412846	41.665895
3522.757412	925939.449975	41.670900
3522.453307	925516.503195	41.675904
3522.364418	925108.194699	41.680909
3522.196193	924682.564337	41.685914
3522.049201	924283.239064	41.690919
3522.110931	923856.447774	41.695924
3522.013950	923444.071973	41.700928
3521.618414	923047.291979	41.705933
3521.763206	922632.506261	41.710938
3521.721268	922228.202618	41.715943
3521.692795	921823.096966	41.720948
3521.851508	921416.294815	41.725952
3521.443230	921014.653931	41.730957
3521.493731	920617.621659	41.735962
3520.940781	920222.199054	41.740967
3521.013547	919821.159962	41.745972
3521.010654	919427.609302	41.750976
3521.005442	919038.553413	41.755981
3520.906018	918629.563406	41.760986
3520.784312	918246.821816	41.765991
3520.869427	917856.800132	41.770996
3520.835627	917466.962586	41.776000
3520.272538	917082.671580	41.781005
3520.595077	916697.148514	41.786010
3520.464831	916319.182727	41.791015
3520.048372	915934.208866	41.796020
3520.161045	915553.068756	41.801024
3519.846743	915173.705823	41.806029
3520.031909	914802.613074	41.811034
3520.078497	914417.070774	41.816039
3519.646547	914052.963519	41.821044
3519.989422	913672.232346	41.826048
3519.459146	913308.477124	41.831053
3519.571136	912937.848102	41.836058
3519.260801	912566.203816	41.841063
3519.293902	912198.813724	41.846068
3519.540252	911843.794405	41.851072
3518.806606	911481.782527	41.856077
3518.631497	911120.522165	41.861082
3518.671317	910761.901313	41.866087
3518.675770	910407.214751	41.871092
3518.847407	910068.382394	41.876096
3518.841755	909713.652925	41.881101
3518.786165	909351.293028	41.886106
3518.460124	909004.765136	41.891111
3518.376410	908652.679912	41.896116
3518.475979	908302.181269	41.901120
3518.316569	907953.728105	41.906125
3518.207616	907604.280381	41.911130
3518.217721	907265.206545	41.916135
3517.969503	906924.900761	41.921140
3517.908250	906563.613259	41.926144
3517.554104	906239.101034	41.931149
3517.556935	905899.945075	41.936154
3517.752233	905564.788456	41.941159
3517.662202	905225.220819	41.946164
3518.128966	904894.899423	41.951168
3517.446004	904566.870594	41.956173
3517.525336	904221.231742	41.961178
3517.149671	903897.648097	41.966183
3517.173802	903580.445591	41.971188
3517.180403	903242.767996	41.976192
3516.978607	902919.678153	41.981197
3516.822067	902603.801250	41.986202
3516.863846	902267.699892	41.991207
3516.729043	901956.126580	41.996212
3516.903584	901640.333898	42.001216
3516.153371	901334.523137	42.006221
3516.711408	901007.336201	42.011226
3516.540987	900688.650399	42.016231
3516.330112	900387.816575	42.021236
3516.409140	900059.301584	42.026240
3516.187251	899751.965774	42.031245
3516.117964	899454.148951	42.036250
3515.902785	899131.422794	42.041255
3515.809728	898836.957591	42.046260
3515.927701	898529.788915	42.051264
3515.859184	898231.134677	42.056269
3515.820047	897926.180762	42.061274
3515.418642	897632.476368	42.066279
3515.312521	897339.191125	42.071284
3515.626205	897040.894111	42.076288
3515.411870	896744.987287	42.081293
3515.381149	896455.701948	42.086298
3515.451612	896167.931273	42.091303
3514.928315	895858.694025	42.096308
3515.233356	895562.060093	42.101312
3515.057483	895283.659354	42.106317
3515.128877	894991.866443	42.111322
3515.044010	894699.697681	42.116327
3515.018187	894405.280991	42.121332
3515.086557	894128.523365	42.126336
3514.657788	893852.124208	42.131341
3514.638878	893558.339293	42.136346
3514.677402	893292.180226	42.141351
3514.501875	893009.994418	42.146356
3514.525408	892724.087673	42.151360
3514.266621	892449.816412	42.156365
3514.673589	892170.877467	42.161370
3514.670584	891901.662792	42.166375
3514.418069	891628.995078	42.171380
3514.547709	891348.901267	42.176384
3514.113345	891077.397792	42.181389
3514.000882	890801.572659	42.186394
3513.751017	890534.365537	42.191399
3513.896557	890273.948703	42.196404
3514.198433	890003.337112	42.201408
3513.924209	889746.254500	42.206413
3513.957949	889476.242696	42.211418
3513.990477	889212.313572	42.216423
3513.887659	888950.619954	42.221428
3513.894362	888669.641654	42.226432
3513.237374	888412.756003	42.231437
3513.420578	888139.366943	42.236442
3513.524980	887901.105717	42.241447
3513.388835	887645.164513	42.246452
3513.383220	887371.092723	42.251456
3513.337208	887125.565795	42.256461
3513.318496	886874.603821	42.261466
3513.082083	886628.506412	42.266471
3512.799565	886380.083016	42.271476
3513.122404	886132.904416	42.276480
3512.712254	885890.385826	42.281485
3512.878764	885635.757829	42.286490
3512.585155	885382.259388	42.291495
3512.484878	885142.853262	42.296500
3512.644867	884900.392929	42.301504
3512.618249	884658.146860	42.306509
3512.762869	884425.254858	42.311514
3512.511492	884183.219660	42.316519
3512.257979	883948.340643	42.321524
3512.499579	883711.240069	42.326528
3512.417575	883461.787034	42.331533
3512.387075	883225.098856	42.336538
3512.195429	882994.141905	42.341543
3511.871053	882760.485682	42.346548
3511.965976	882531.690877	42.351552
3511.738316	882310.883082	42.356557
3511.962471	882076.043545	42.361562
3511.964607	881856.536841	42.366567
3511.753399	881633.666403	42.371572
3511.557466	881408.556728	42.376576
3511.447167	881183.036738	42.381581
3511.852612	880958.973257	42.386586
3511.695019	880729.665005	42.391591
3511.442160	880517.319865	42.396596
3511.631204	880294.526212	42.401600
3511.274639	880088.093318	42.406605
3511.370546	879854.542285	42.411610
3511.424592	879641.630304	42.416615
3511.054882	879412.983793	42.421620
3511.210425	879207.307707	42.426624
3510.984416	879005.564022	42.431629
3511.333122	878786.466587	42.436634
3511.103440	878570.364048	42.441639
3510.489720	878356.740064	42.446644
3510.943956	878159.992513	42.451648
3510.792428	877951.221200	42.456653
3510.935519	877751.021540	42.461658
3510.916261	877539.111756	42.466663
3510.918345	877338.630477	42.471668
3511.174987	877127.726843	42.476672
3510.706978	876917.710678	42.481677
3510.592837	876717.615230	42.486682
3510.771718	876510.871461	42.491687
3510.630248	876310.378864	42.496692
3510.740240	876103.826113	42.501696
3510.522480	875902.653472	42.506701
3510.604597	875704.042842	42.511706
3510.411238	875504.113257	42.516711
3510.404139	875309.383113	42.521716
3510.471252	875109.009337	42.526720
3510.247511	874909.064640	42.531725
3510.109178	874707.741265	42.536730
3510.142666	874528.593993	42.541735
3510.348533	874329.625862	42.546740
3510.485459	874130.274417	42.551744
3510.047625	873943.136200	42.556749
3510.079905	873745.244078	42.561754
3509.857101	873558.252297	42.566759
3509.735831	873366.678369	42.571764
3509.790674	873181.957258	42.576768
3509.767264	872993.653657	42.581773
3509.635955	872811.086064	42.586778
3509.564231	872627.726860	42.591783
3509.616884	872448.610665	42.596788
3509.622363	872254.748405	42.601792
3509.719259	872078.815756	42.606797
3509.791092	871886.968263	42.611802
3509.705910	871716.488886	42.616807
3509.300477	871533.830226	42.621812
3509.489009	871344.469105	42.626816
3509.110835	871178.971871	42.631821
3508.828860	870997.052793	42.636826
3508.994822	870836.988257	42.641831
3508.741578	870673.591568	42.646836
3509.198573	870489.302994	42.651840
3508.672182	870323.029969	42.656845
3509.056081	870162.620271	42.661850
3508.900533	869993.268002	42.666855
3508.716358	869823.527375	42.671860
3508.996138	869645.163177	42.676864
3508.573475	869485.353560	42.681869
3508.575714	869325.469666	42.686874
3508.592592	869168.879795	42.691879
3508.471191	869010.172806	42.696884
3508.581353	868835.695723	42.701888
3508.430761	868679.411903	42.706893
3508.446800	868517.562422	42.711898
3508.464933	868366.582600	42.716903
3508.205159	868220.596606	42.721908
3508.842340	868058.535310	42.726912
3508.629088	867901.173461	42.731917
3508.723412	867727.831965	42.736922
3508.332132	867568.160248	42.741927
3508.149717	867421.559441	42.746932
3507.947239	867264.858896	42.751936
3508.191448	867114.587228	42.756941
3508.140099	866955.231667	42.761946
3507.875938	866814.262204	42.766951
3508.137338	866656.886683	42.771956
3508.204869	866505.851962	42.776960
3507.873743	866365.757127	42.781965
3507.896989	866205.398173	42.786970
3508.092281	866051.514313	42.791975
3508.068017	865901.742258	42.796980
3507.886466	865746.649982	42.801985
3507.859635	865606.973040	42.806989
3507.828497	865460.105259	42.811994
3507.456966	865323.101298	42.816999
3507.482477	865171.068638	42.822004
3507.847637	865021.404853	42.827009
3507.575123	864887.871972	42.832013
3507.653595	864752.918198	42.837018
3507.825850	864615.322828	42.842023
3507.385902	864468.984057	42.847028
3507.781372	864325.321675	42.852033
3507.714647	864186.978670	42.857037
3507.837804	864030.043220	42.862042
3507.675767	863881.312539	42.867047
3507.074398	863759.760175	42.872052
3507.220267	863615.441900	42.877057
3507.327526	863494.350470	42.882061
3507.425737	863346.146790	42.887066
3507.253065	863209.936725	42.892071
3507.036423	863078.298196	42.897076
3507.250066	862935.798947	42.902081
3506.981641	862810.771376	42.907085
3507.169697	862679.932160	42.912090
3507.283400	862552.017959	42.917095
3506.842871	862406.892856	42.922100
3507.219874	862287.287898	42.927105
3507.373816	862161.108260	42.932109
3507.347642	862020.765276	42.937114
3507.390178	861889.641427	42.942119
3507.190588	861762.539791	42.947124
3507.166992	861611.106253	42.952129
3507.092662	861494.087281	42.957133
3507.349803	861366.999331	42.962138
3507.046716	861221.337233	42.967143
3507.054949	861095.159482	42.972148
3506.846086	860973.292185	42.977153
3506.912007	860855.071281	42.982157
3506.827918	860728.998365	42.987162
3507.008306	860606.184653	42.992167
3506.810554	860484.791836	42.997172
3506.827372	860353.444687	43.002177
3506.766183	860218.801965	43.007181
3506.664603	860097.677263	43.012186
3506.699636	859982.166826	43.017191
3506.239198	859863.624506	43.022196
3506.797040	859729.646831	43.027201
3506.321482	859621.603260	43.032205
3506.481819	859486.713419	43.037210
3506.443654	859384.135977	43.042215
3506.409617	859261.913956	43.047220
3506.236344	859139.031745	43.052225
3506.328698	859043.136673	43.057229
3506.118394	858924.437659	43.062234
3506.366269	858808.772719	43.067239
3505.968164	858706.826687	43.072244
3506.005379	858584.093136	43.077249
3506.048297	858468.066527	43.082253
3505.786337	858363.952818	43.087258
3506.061229	858252.746552	43.092263
3505.831826	858145.025330	43.097268
3505.886626	858042.021034	43.102273
3506.079608	857939.964836	43.107277
3505.827487	857827.476045	43.112282
3505.859049	857710.367076	43.117287
3505.645263	857621.114067	43.122292
3505.714955	857511.873461	43.127297
3506.018368	857416.890810	43.132301
3505.979138	857298.618424	43.137306
3506.012735	857190.837097	43.142311
3505.898585	857092.027351	43.147316
3505.887544	856975.786834	43.152321
3505.912045	856881.133672	43.157325
3505.541603	856775.162588	43.162330
3506.020436	856663.893918	43.167335
3505.661467	856567.645344	43.172340
3505.528511	856460.754174	43.177345
3505.600551	856361.999287	43.182349
3505.786356	856256.122171	43.187354
3505.596351	856173.946095	43.192359
3505.427776	856073.669617	43.197364
3505.908281	855958.885504	43.202369
3505.592420	855859.700005	43.207373
3505.477446	855761.160868	43.212378
3505.177897	855660.120873	43.217383
3505.201742	855569.728638	43.222388
3505.494764	855480.361013	43.227393
3505.198470	855383.207878	43.232397
3505.368814	855283.446483	43.237402
3505.106110	855205.939935	43.242407
3504.940742	855111.582728	43.247412
3505.395922	855019.165260	43.252417
3505.329856	854927.513439	43.257421
3505.419951	854827.855200	43.262426
3505.558111	854736.361508	43.267431
3505.374974	854634.312399	43.272436
3505.099919	854541.229589	43.277441
3505.191904	854458.302957	43.282445
3505.223929	854367.599801	43.287450
3505.428587	854274.628564	43.292455
3504.922119	854188.293469	43.297460
3505.104806	854093.668703	43.302465
3505.371130	854018.298433	43.307469
3505.048643	853916.747024	43.312474
3505.188232	853829.619204	43.317479
3505.137554	853734.248786	43.322484
3505.467303	853640.176805	43.327489
3505.369210	853551.332325	43.332493
3505.066344	853464.466915	43.337498
3505.374014	853378.375679	43.342503
3504.858542	853286.092208	43.347508
3505.127777	853194.554084	43.352513
3504.466560	853105.601308	43.357517
3504.724407	853027.397613	43.362522
3504.795174	852944.940858	43.367527
3504.849763	852859.565472	43.372532
3504.707057	852770.717129	43.377537
3504.739173	852697.510866	43.382541
3504.792265	852609.504032	43.387546
3504.912449	852528.591094	43.392551
3504.561158	852451.745979	43.397556
3504.462051	852369.990981	43.402561
3504.590094	852296.764178	43.407565
3504.287499	852219.616112	43.412570
3504.540462	852136.729181	43.417575
3504.679715	852063.497776	43.422580
3504.719529	851979.280926	43.427585
3504.482687	851903.091625	43.432589
3504.501594	851824.425346	43.437594
3504.576449	851742.633414	43.442599
3504.561959	851666.891364	43.447604
3504.474972	851584.734581	43.452609
3504.555237	851517.932210	43.457613
3504.746171	851441.179951	43.462618
3504.644148	851366.130189	43.467623
3504.331089	851284.590860	43.472628
3504.666802	851209.564450	43.477633
3504.669206	851136.636757	43.482637
3504.694235	851056.207131	43.487642
3504.613420	850969.270143	43.492647
3504.364478	850894.433626	43.497652
3504.420721	850818.961694	43.502657
3504.314321	850747.605312	43.507661
3504.378622	850665.800941	43.512666
3504.573380	850594.685310	43.517671
3504.493342	850533.351791	43.522676
3504.466287	850455.746894	43.527681
3504.355533	850383.802789	43.532685
3504.293912	850313.505216	43.537690
3504.581656	850235.066662	43.542695
3504.421019	850156.408848	43.547700
3504.739385	850075.333915	43.552705
3504.682603	850007.174524	43.557709
3504.368238	849924.351565	43.562714
3504.460399	849843.116107	43.567719
3504.691519	849770.134712	43.572724
3504.804103	849696.490266	43.577729
3504.364260	849617.969041	43.582733
3504.194311	849543.298036	43.587738
3504.466295	849479.266551	43.592743
3504.169513	849398.868528	43.597748
3504.430508	849330.259798	43.602753
3504.347873	849264.044441	43.607757
3504.374317	849188.655056	43.612762
3504.403247	849109.173607	43.617767
3504.076430	849048.158317	43.622772
3504.380380	848971.941395	43.627777
3504.666648	848904.882239	43.632781
3504.565089	848821.619954	43.637786
3504.706553	848745.037422	43.642791
3504.046550	848677.449899	43.647796
3504.306393	848610.586749	43.652801
3504.706329	848533.277190	43.657805
3504.220710	848459.132253	43.662810
3504.434860	848387.696031	43.667815
3504.338271	848311.926690	43.672820
3503.974563	848241.168466	43.677825
3504.075280	848172.768254	43.682829
3504.160655	848100.181004	43.687834
3504.212417	848042.600425	43.692839
3504.039565	847972.002538	43.697844
3503.998056	847896.706170	43.702849
3503.956262	847837.190763	43.707853
3504.082320	847777.744553	43.712858
3504.183419	847706.806278	43.717863
3503.857226	847642.562267	43.722868
3503.992365	847584.379205	43.727873
3504.092688	847524.739988	43.732877
3503.856228	847459.407654	43.737882
3504.410300	847389.560245	43.742887
3504.109971	847312.253553	43.747892
3503.966108	847239.206951	43.752897
3504.175907	847183.833274	43.757901
3503.773974	847113.848017	43.762906
3503.797554	847052.268349	43.767911
3503.960889	846993.490569	43.772916
3503.843363	846930.179181	43.777921
3504.024676	846859.510391	43.782925
3503.731358	846805.872641	43.787930
3503.846493	846746.321008	43.792935
3503.838331	846680.260882	43.797940
3504.112979	846627.210081	43.802945
3504.010575	846560.579597	43.807949
3503.798291	846496.499933	43.812954
3503.870296	846424.577541	43.817959
3503.699926	846369.161866	43.822964
3503.753842	846302.113116	43.827969
3503.791257	846243.738827	43.832973
3503.777860	846177.771715	43.837978
3503.780338	846114.529763	43.842983
3503.667932	846070.892774	43.847988
3503.878360	846015.216342	43.852993
3503.794964	845958.321006	43.857997
3503.693537	845892.170501	43.863002
3503.668312	845820.939354	43.868007
3503.386086	845774.989490	43.873012
3503.753488	845708.759810	43.878017
3503.429414	845666.129397	43.883021
3503.428897	845602.200614	43.888026
3503.685743	845548.364009	43.893031
3503.467306	845504.058372	43.898036
3503.676729	845437.169677	43.903041
3503.632553	845376.364375	43.908045
3503.383864	845316.176926	43.913050
3503.572494	845263.810992	43.918055
3503.649913	845215.361315	43.923060
3503.770726	845149.166373	43.928065
3503.547609	845097.256732	43.933069
3503.330982	845039.108030	43.938074
3503.584124	844985.657070	43.943079
3503.309174	844935.216573	43.948084
3503.408934	844882.959576	43.953089
3503.406769	844820.874945	43.958093
3503.200764	844773.735614	43.963098
3503.477837	844714.722843	43.968103
3502.936773	844672.023968	43.973108
3503.411108	844616.194205	43.978113
3503.447556	844574.959017	43.983117
3503.345113	844517.858844	43.988122
3503.328546	844473.025331	43.993127
3503.167426	844420.904952	43.998132
3503.235827	844369.136216	44.003137
3503.517226	844320.548574	44.008141
3502.889461	844268.796240	44.013146
3503.368933	844220.857513	44.018151
3503.359933	844176.313065	44.023156
3503.552844	844119.745474	44.028161
3503.599200	844069.050144	44.033165
3503.477879	844018.674466	44.038170
3503.689293	843957.910831	44.043175
3503.493025	843900.918005	44.048180
3503.570682	843837.738259	44.053185
3503.529339	843802.359664	44.058189
3503.554717	843749.813084	44.063194
3503.470302	843693.482327	44.068199
3503.430359	843644.552494	44.073204
3503.369090	843592.993718	44.078209
3503.409635	843537.713310	44.083213
3503.416946	843496.865812	44.088218
3503.628891	843432.685028	44.093223
3503.441712	843378.903051	44.098228
3503.503874	843329.076561	44.103233
3503.672986	843276.892315	44.108237
3503.174157	843214.288757	44.113242
3503.520812	843166.753877	44.118247
3503.114715	843124.314736	44.123252
3503.670854	843060.463428	44.128257
3503.489633	843001.900120	44.133261
3503.202363	842963.925020	44.138266
3503.261408	842902.493875	44.143271
3503.226860	842861.064192	44.148276
3503.412532	842810.238304	44.153281
3503.226018	842774.390384	44.158285
3503.220480	842711.213076	44.163290
3503.475120	842657.449658	44.168295
3503.125145	842618.800322	44.173300
3503.148401	842560.979231	44.178305
3503.327890	842517.562027	44.183309
3503.282549	842463.748887	44.188314
3503.061831	842408.209137	44.193319
3503.081075	842376.712677	44.198324
3503.051568	842319.483091	44.203329
3503.097246	842276.671305	44.208333
3503.091886	842241.960573	44.213338
3503.223788	842186.068260	44.218343
3502.854557	842151.124463	44.223348
3503.029652	842097.710670	44.228353
3503.579471	842054.863076	44.233357
3503.226080	842001.145510	44.238362
3503.295718	841958.278869	44.243367
3503.418752	841909.942566	44.248372
3503.173103	841862.788015	44.253377
3503.434471	841811.892885	44.258381
3503.303980	841768.229081	44.263386
3503.375664	841717.364444	44.268391
3503.493371	841674.487963	44.273396
3503.393420	841622.431918	44.278401
3503.446623	841568.546175	44.283405
3503.280446	841509.722782	44.288410
3503.168564	841467.906653	44.293415
3503.169524	841415.783526	44.298420
3502.992783	841366.761086	44.303425
3502.924355	841331.275606	44.308429
3502.859262	841286.817554	44.313434
3503.163066	841236.934777	44.318439
3502.853815	841201.244445	44.323444
3503.110012	841157.854047	44.328449
3503.185625	841115.078241	44.333453
3503.222520	841070.553109	44.338458
3503.288028	841018.269795	44.343463
3503.510196	840972.884498	44.348468
3503.334530	840921.907947	44.353473
3503.413088	840868.792285	44.358477
3503.150732	840822.461716	44.363482
3503.460731	840771.355174	44.368487
3503.502654	840731.947046	44.373492
3503.545304	840686.540516	44.378497
3503.685419	840624.732574	44.383501
3503.174507	840579.465248	44.388506
3503.639067	840517.212681	44.393511
3503.519602	840479.048720	44.398516
3503.408462	840420.108620	44.403521
3503.386826	840371.199231	44.408525
3503.321302	840321.516418	44.413530
3503.230942	840262.766503	44.418535
3503.073617	840224.168337	44.423540
3503.207918	840170.842583	44.428545
3503.395042	840125.652083	44.433549
3503.250309	840080.711016	44.438554
3503.030055	840023.492135	44.443559
3503.050828	839992.617588	44.448564
3503.182971	839941.582450	44.453569
3503.255216	839902.603115	44.458573
3502.837758	839848.975405	44.463578
3503.341749	839810.899793	44.468583
3503.242489	839770.533539	44.473588
3502.990337	839725.071168	44.478593
3502.815172	839673.011525	44.483597
3503.035709	839632.055206	44.488602
3503.174217	839582.479320	44.493607
3503.239826	839551.595245	44.498612
3503.326275	839493.052953	44.503617
3503.304022	839452.915864	44.508621
3503.356635	839399.597105	44.513626
3503.428743	839341.884951	44.518631
3503.303005	839301.471308	44.523636
3503.116076	839250.580751	44.528641
3502.971555	839195.195410	44.533645
3503.078266	839166.692720	44.538650
3503.260427	839121.837347	44.543655
3503.052303	839075.631431	44.548660
3503.016982	839025.250640	44.553665
3503.347861	839007.490078	44.558669
3502.888846	838948.252209	44.563674
3502.880780	838896.744020	44.568679
3502.992352	838868.385530	44.573684
3503.122330	838827.487740	44.578689
3502.743781	838779.893171	44.583693
3502.895341	838736.991299	44.588698
3503.021911	838687.215295	44.593703
3502.879308	838661.580657	44.598708
3502.802020	838610.130336	44.603713
3502.923572	838577.427445	44.608717
3502.819145	838537.054221	44.613722
3502.979185	838489.466306	44.618727
3503.106669	838442.224873	44.623732
3502.866901	838413.922250	44.628737
3503.150212	838377.776945	44.633741
3503.054381	838323.400431	44.638746
3503.159683	838275.478461	44.643751
3502.872304	838244.207163	44.648756
3503.003307	838198.817112	44.653761
3503.054109	838146.610194	44.658765
3502.845968	838116.105757	44.663770
3502.836256	838068.396319	44.668775
3502.806012	838032.203151	44.673780
3503.085319	837985.469958	44.678785
3502.770045	837956.299608	44.683789
3502.911772	837914.906180	44.688794
3503.253331	837864.307766	44.693799
3503.002569	837830.784242	44.698804
3502.941522	837793.911790	44.703809
3503.138839	837747.970956	44.708813
3503.061780	837707.929485	44.713818
3503.232343	837647.990351	44.718823
3502.779878	837616.060142	44.723828
3503.110645	837563.851122	44.728833
3503.038054	837525.856889	44.733837
3503.010292	837485.903482	44.738842
3502.988627	837436.386097	44.743847
3502.897626	837397.223185	44.748852
3502.831552	837357.519236	44.753857
3502.932130	837318.714600	44.758861
3502.745527	837280.396159	44.763866
3503.153580	837236.807673	44.768871
3503.043602	837193.743364	44.773876
3503.171159	837151.615460	44.778881
3503.166866	837113.656316	44.783885
3502.535783	837078.386202	44.788890
3502.924120	837028.749316	44.793895
3502.666363	837001.907168	44.798900
3502.810948	836955.530197	44.803905
3502.976432	836917.981057	44.808909
3502.823475	836883.216609	44.813914
3502.779127	836837.699405	44.818919
3502.736346	836802.867573	44.823924
3502.998985	836755.591406	44.828929
3502.872858	836714.136750	44.833933
3502.687010	836683.816976	44.838938
3502.778498	836642.130819	44.843943
3502.537038	836606.598721	44.848948
3502.853905	836566.631587	44.853953
3502.799132	836528.091733	44.858957
3502.855651	836482.896962	44.863962
3502.853565	836455.961600	44.868967
3502.743650	836410.842539	44.873972
3502.624836	836379.534333	44.878977
3502.624042	836343.131563	44.883981
3502.399621	836307.253410	44.888986
3502.842164	836267.898083	44.893991
3502.424482	836234.540080	44.898996
3502.656154	836202.831674	44.904001
3503.058557	836160.944764	44.909005
3503.074328	836133.077919	44.914010
3503.202741	836099.775637	44.919015
3502.973778	836048.573683	44.924020
3502.981951	836007.726726	44.929025
3502.877732	835959.529127	44.934029
3502.779261	835925.482511	44.939034
3502.655848	835886.120488	44.944039
3502.632560	835852.451507	44.949044
3502.616202	835810.240891	44.954049
3502.871924	835771.157310	44.959053
3502.351004	835744.987673	44.964058
3502.347837	835702.383756	44.969063
3502.325598	835687.697941	44.974068
3502.440454	835654.688399	44.979073
3502.976507	835621.902111	44.984077
3502.501469	835583.035391	44.989082
3502.632103	835527.426506	44.994087
3502.946768	835507.121113	44.999092
3502.565653	835467.994199	45.004097
3503.027857	835429.216148	45.009101
3502.348792	835401.997460	45.014106
3502.695504	835361.871493	45.019111
3502.528197	835326.320074	45.024116
3502.674061	835293.352372	45.029121
3502.688095	835250.156950	45.034125
3502.454064	835227.207935	45.039130
3502.699335	835170.649755	45.044135
3502.702545	835161.815344	45.049140
3502.630949	835130.151609	45.054145
3502.786671	835090.738716	45.059149
3502.791788	835063.991551	45.064154
3502.641759	835010.425541	45.069159
3502.696275	834990.795884	45.074164
3502.166973	834940.757153	45.079169
3502.622606	834911.933981	45.084173
3502.457781	834886.336676	45.089178
3502.617545	834842.431178	45.094183
3502.395879	834815.769154	45.099188
3502.711200	834776.181608	45.104193
3502.519170	834743.803666	45.109197
3502.348778	834720.110202	45.114202
3502.166126	834674.502810	45.119207
3502.755142	834665.961684	45.124212
3502.414115	834628.140925	45.129217
3502.667608	834588.513602	45.134221
3502.448827	834569.562232	45.139226
3502.635749	834524.673865	45.144231
3502.582380	834493.150423	45.149236
3502.819869	834453.280845	45.154241
3502.802020	834425.412128	45.159245
3502.492099	834388.463455	45.164250
3502.599746	834353.642352	45.169255
3502.441993	834313.739404	45.174260
3502.846592	834277.990329	45.179265
3503.037614	834244.521676	45.184269
3502.770611	834203.610957	45.189274
3502.594893	834173.619341	45.194279
3502.654455	834144.711554	45.199284
3502.519503	834107.488366	45.204289
3502.628832	834073.055987	45.209293
3502.182089	834041.936850	45.214298
3502.778760	834015.917721	45.219303
3502.552332	833983.736879	45.224308
3502.406114	833964.234795	45.229313
3502.439507	833909.994788	45.234317
3502.309390	833894.834487	45.239322
3502.738650	833855.027242	45.244327
3502.386363	833830.677035	45.249332
3502.337704	833792.998458	45.254337
3502.474325	833769.787896	45.259341
3502.386546	833742.074194	45.264346
3502.606455	833700.103697	45.269351
3502.537322	833678.098334	45.274356
3502.510779	833650.667057	45.279361
3502.567797	833610.919637	45.284365
3502.269456	833584.509230	45.289370
3502.576918	833551.603619	45.294375
3502.152907	833525.555409	45.299380
3502.346002	833478.168955	45.304385
3502.428944	833455.307842	45.309389
3502.238848	833432.735733	45.314394
3502.298825	833405.484437	45.319399
3502.412261	833380.177029	45.324404
3502.259948	833341.829407	45.329409
3502.393533	833324.525029	45.334413
3502.195045	833283.645992	45.339418
3502.802045	833259.282032	45.344423
3502.497718	833224.962098	45.349428
3502.429664	833208.178845	45.354433
3502.355053	833158.881289	45.359437
3502.230840	833152.408567	45.364442
3502.762050	833110.627056	45.369447
3502.703602	833080.269269	45.374452
3502.709499	833032.422158	45.379457
3502.549476	832996.612544	45.384461
3502.418070	832982.426770	45.389466
3502.556926	832945.054104	45.394471
3502.278859	832913.071712	45.399476
3502.052404	832886.158357	45.404481
3502.459845	832852.305055	45.409485
3502.593346	832830.556357	45.414490
3502.600405	832791.398012	45.419495
3502.271973	832762.255004	45.424500
3502.283254	832741.844418	45.429505
3502.587456	832705.712578	45.434509
3502.326504	832679.145820	45.439514
3502.345714	832646.722523	45.444519
3502.205601	832612.421095	45.449524
3502.186346	832589.622581	45.454529
3502.446600	832559.014526	45.459533
3502.466237	832550.759745	45.464538
3502.561714	832501.722104	45.469543
3501.908252	832480.785466	45.474548
3502.371841	832456.881560	45.479553
3502.569490	832420.228580	45.484557
3502.208633	832397.436842	45.489562
3502.484147	832366.239428	45.494567
3502.233692	832344.015247	45.499572
3502.102688	832309.954852	45.504577
3502.482971	832281.327670	45.509581
3502.252546	832251.287290	45.514586
3502.326488	832216.264886	45.519591
3502.718637	832213.417154	45.524596
3502.343124	832185.402364	45.529601
3502.707214	832143.105017	45.534605
3502.309817	832111.675438	45.539610
3502.430583	832074.935508	45.544615
3502.322827	832057.569842	45.549620
3502.271343	832020.906816	45.554625
3502.131884	831993.780082	45.559629
3502.185575	831974.092545	45.564634
3502.395582	831935.042064	45.569639
3502.357016	831917.664622	45.574644
3502.291814	831886.765190	45.579649
3502.180244	831858.851990	45.584653
3502.249760	831829.883361	45.589658
3502.754764	831799.719710	45.594663
3502.520286	831768.310448	45.599668
3502.361767	831743.285599	45.604673
3502.411945	831707.043538	45.609677
3502.206798	831689.644095	45.614682
3502.488957	831655.561011	45.619687
3502.432893	831623.877485	45.624692
3502.275990	831603.588682	45.629697
3502.639746	831554.939163	45.634701
3502.224869	831544.117647	45.639706
3502.416759	831499.207421	45.644711
3502.287937	831482.087851	45.649716
3502.311710	831461.036313	45.654721
3502.385932	831430.160563	45.659725
3502.341957	831402.038914	45.664730
3502.635622	831370.443031	45.669735
3502.424526	831336.586045	45.674740
3502.248344	831311.220583	45.679745
3502.418274	831272.807580	45.684749
3502.220833	831260.387002	45.689754
3502.333563	831229.943480	45.694759
3502.553825	831214.865658	45.699764
3502.108757	831190.032390	45.704769
3502.666218	831150.919935	45.709773
3502.312283	831132.664439	45.714778
3502.403083	831085.814513	45.719783
3502.416568	831072.186719	45.724788
3502.371969	831032.928560	45.729793
3502.433938	831012.455327	45.734797
3502.329133	830975.599810	45.739802
3502.323971	830949.081468	45.744807
3502.387724	830915.128153	45.749812
3502.256820	830896.591048	45.754817
3502.409593	830845.968571	45.759821
3502.233950	830769.172781	45.764826
3502.349177	830617.064388	45.769831
3502.489327	830420.990110	45.774836
3502.099085	830164.186108	45.779841
3502.217736	829839.049192	45.784845
3501.738317	829464.949512	45.789850
3502.086156	829035.830262	45.794855
3502.124409	828540.582014	45.799860
3501.881993	827985.683446	45.804865
3501.726003	827358.940222	45.809869
3501.423325	826679.185380	45.814874
3501.197974	825920.803280	45.819879
3501.029062	825117.401319	45.824884
3500.389504	824245.387813	45.829889
3500.319502	823309.111543	45.834893
3499.916150	822308.449642	45.839898
3499.829865	821226.733966	45.844903
3499.258506	820100.893842	45.849908
3498.916218	818882.350486	45.854913
3498.800789	817588.818379	45.859917
3498.074269	816251.425629	45.864922
3497.683128	814813.395066	45.869927
3497.113676	813319.358652	45.874932
3496.525493	811746.624795	45.879937
3496.003452	810110.264427	45.884941
3495.361550	808403.794850	45.889946
3495.143062	806612.173944	45.894951
3494.427709	804754.855431	45.899956
3493.907680	802829.515849	45.904961
3493.119085	800810.273643	45.909965
3492.780516	798726.276907	45.914970
3491.804509	796580.005740	45.919975
3490.939664	794351.542313	45.924980
3490.242622	792044.191740	45.929985
3489.605778	789681.582346	45.934989
3488.573811	787237.637262	45.939994
3488.095413	784723.184535	45.944999
3487.019067	782144.493385	45.950004
3486.333139	779484.902072	45.955009
3485.648596	776752.415361	45.960013
3484.526540	773973.819038	45.965018
3483.476730	771098.882421	45.970023
3482.548103	768163.469096	45.975028
3481.623821	765161.470345	45.980033
3480.842974	762088.451117	45.985037
3479.508010	758958.363445	45.990042
3478.321807	755752.469364	45.995047
3477.493640	752477.810140	46.000052
3476.366727	749138.172152	46.005057
3475.519825	745714.802517	46.010061
3473.517893	742249.279610	46.015066
3472.600573	738715.070131	46.020071
3471.712139	735110.735898	46.025076
3470.631524	731441.580977	46.030081
3468.807586	727691.819769	46.035085
3467.316004	723903.704829	46.040090
3466.634130	720038.989731	46.045095
3465.342642	716112.404277	46.050100
3463.860786	712112.444790	46.055105
3462.506228	708045.379892	46.060109
3460.867326	703935.743997	46.065114
3459.509933	699742.696428	46.070119
3457.977168	695494.062098	46.075124
3456.478226	691192.037700	46.080129
3455.468962	686819.769758	46.085133
3453.650616	682371.867116	46.090138
3452.084958	677875.075064	46.095143
3450.347668	673319.050274	46.100148
3448.554217	668707.006382	46.105153
3446.766957	664026.704648	46.110157
3445.253203	659289.113511	46.115162
3443.325695	654478.110301	46.120167
3442.107547	649618.569760	46.125172
3440.408656	644693.501547	46.130177
3438.563135	639715.443892	46.135181
3436.457996	634677.817424	46.140186
3434.832702	629573.640454	46.145191
3432.835211	624427.489938	46.150196
3430.663400	619225.679206	46.155201
3429.050439	613964.135922	46.160205
3426.944393	608651.717529	46.165210
3424.725329	603277.239033	46.170215
3422.802489	597844.605179	46.175220
3420.529511	592370.312141	46.180225
3418.819733	586837.761859	46.185229
3416.500867	581263.907661	46.190234
3414.286929	575620.049493	46.195239
3412.115801	569938.662750	46.200244
3409.675643	564214.159027	46.205249
3407.867279	558414.447492	46.210253
3405.109677	552580.611505	46.215258
3402.665558	546698.637890	46.220263
3400.619955	540766.487828	46.225268
3398.172617	534784.991719	46.230273
3395.884727	528754.910249	46.235277
3393.022403	522688.128851	46.240282
3390.570594	516570.253132	46.245287
3387.940561	510405.523646	46.250292
3385.351998	504214.487874	46.255297
3382.930768	497957.049002	46.260301
3379.983760	491672.167857	46.265306
3377.432133	485348.945783	46.270311
3374.831457	478987.277531	46.275316
3371.754632	472580.776090	46.280321
3369.299584	466132.169703	46.285325
3366.035142	459660.676268	46.290330
3363.243720	453131.908940	46.295335
3360.467481	446582.474442	46.300340
3357.261908	440005.598984	46.305345
3354.564362	433387.423507	46.310349
3351.597892	426732.123470	46.315354
3348.459125	420063.437160	46.320359
3345.219567	413347.998963	46.325364
3342.007127	406606.096159	46.330369
3339.332480	399844.459391	46.335373
3335.594647	393064.610055	46.340378
3332.652634	386242.872083	46.345383
3329.380992	379397.964763	46.350388
3325.404534	372518.725239	46.355393
3322.185176	365629.286202	46.360397
3318.508836	358712.346269	46.365402
3315.253794	351789.656400	46.370407
3311.519806	344859.942886	46.375412
3307.988837	337893.804486	46.380417
3304.664903	330925.184783	46.385421
3300.534686	323948.478503	46.390426
3296.887558	316952.606865	46.395431
3293.382812	309941.472075	46.400436
3289.278481	302928.695176	46.405441
3285.880776	295896.116477	46.410445
3281.713039	288876.019473	46.415450
3277.890266	281830.030942	46.420455
3274.080294	274794.502302	46.425460
3270.105236	267748.232395	46.430465
3266.234043	260705.167354	46.435469
3261.644904	253662.548379	46.440474
3257.561728	246614.044898	46.445479
3253.612670	239574.167544	46.450484
3249.495728	232551.301772	46.455489
3245.414248	225489.779537	46.460493
3240.776653	218395.163141	46.465498
3236.309720	211368.890129	46.470503
3232.460967	204366.453636	46.475508
3227.700384	197371.446082	46.480513
3223.643931	190365.826904	46.485517
3218.823466	183411.122496	46.490522
3213.556826	176457.836637	46.495527
3209.272271	169522.507070	46.500532
3204.666432	162619.440305	46.505537
3200.070002	155729.444075	46.510541
3194.858801	148866.580835	46.515546
3190.063358	142037.445949	46.520551
3184.973837	135231.704614	46.525556
3179.986641	128449.063435	46.530561
3175.084635	121700.171537	46.535565
3169.870519	114997.838079	46.540570
3164.676777	108339.016167	46.545575
3159.326144	101714.890436	46.550580
3154.079430	95122.158354	46.555585
3148.712633	88579.424303	46.560589
3142.789529	82089.403816	46.565594
3136.933241	75633.072479	46.570599
3131.183393	69263.021070	46.575604
3125.141906	62925.843929	46.580609
3118.485146	56668.238514	46.585613
3111.672773	50484.627366	46.590618
3104.395656	44380.573427	46.595623
3095.928182	38406.452293	46.600628
3080.969500	32710.345070	46.605633
3062.806683	27245.608986	46.610637
3044.177020	22050.372123	46.615642
3025.465266	17145.436994	46.620647
3004.088891	12658.729756	46.625652
2977.630697	8654.306286	46.630657
2949.516237	5170.071055	46.635661
2920.261807	2230.558432	46.640666
2870.843830	412.118706	46.645671
2785.871693	324.347102	46.650676
2740.110353	324.169913	46.655681
2736.029234	317.835413	46.660685
2757.253656	300.869934	46.665690
2787.122035	295.291395	46.670695
2813.236585	302.456326	46.675700
2829.331512	302.103971	46.680705
2835.520766	293.973490	46.685709
2834.272038	294.898372	46.690714
2829.997260	293.437361	46.695719
2825.014551	286.706092	46.700724
2819.856483	297.619757	46.705729
2816.138573	294.332238	46.710733
2813.043597	299.701594	46.715738
2810.541751	289.237374	46.720743
2808.440427	277.299633	46.725748
2806.265058	284.134681	46.730753
2803.920369	276.289725	46.735757
2801.142159	283.691150	46.740762
2798.101571	292.032991	46.745767
2795.366009	285.399087	46.750772
2791.979114	281.284575	46.755777
2788.656694	281.773691	46.760781
2785.273908	275.183042	46.765786
2782.067004	283.484837	46.770791
2779.385151	278.877870	46.775796
2776.183654	272.161804	46.780801
2773.380360	271.623952	46.785805
2770.098357	269.437553	46.790810
2766.317414	274.393996	46.795815
2763.018761	269.396642	46.800820
2759.789532	277.217062	46.805825
2756.584223	266.395341	46.810829
2753.191348	266.788356	46.815834
2750.188713	264.357349	46.820839
2746.879228	268.408753	46.825844
2743.358852	273.298536	46.830849
2740.400580	264.461983	46.835853
2736.807682	268.969446	46.840858
2733.004168	267.605211	46.845863
2730.213610	268.760847	46.850868
2726.562197	266.211937	46.855873
2723.953789	257.161768	46.860877
2720.437247	264.586777	46.865882
2716.187793	255.294707	46.870887
2712.719447	253.398800	46.875892
2709.565886	266.722467	46.880897
2705.985447	256.394477	46.885901
2702.858068	265.079445	46.890906
2699.227568	262.771020	46.895911
2696.732610	250.220249	46.900916
2693.269116	257.967658	46.905921
2689.528832	254.784582	46.910925
2686.104180	257.708468	46.915930
2682.303015	259.914987	46.920935
2678.928166	256.484141	46.925940
2675.524225	262.041896	46.930945
2672.360407	252.116439	46.935949
2668.709581	250.359609	46.940954
2665.107692	250.922551	46.945959
2661.753589	250.566434	46.950964
2658.196491	255.198284	46.955969
2655.134430	249.837540	46.960973
2651.513159	252.598131	46.965978
2648.308849	249.352690	46.970983
2644.795581	246.396626	46.975988
2641.166414	250.882111	46.980993
2637.662435	240.373435	46.985997
2634.377345	249.247462	46.991002
2631.226516	248.401566	46.996007
2628.052145	239.053736	47.001012
2624.208793	247.211979	47.006017
2620.186454	238.334048	47.011021
2616.617163	238.146482	47.016026
2613.475638	247.071818	47.021031
2610.582412	237.560777	47.026036
2606.407122	251.390946	47.031041
2603.079133	246.100963	47.036045
2599.902218	243.268216	47.041050
2596.553842	243.274307	47.046055
2593.252938	233.268532	47.051060
2589.109507	250.613633	47.056065
2585.076280	239.594399	47.061069
2582.139089	242.826665	47.066074
2579.188932	244.384065	47.071079
2576.289062	238.524964	47.076084
2572.295209	243.854126	47.081089
2568.479255	239.109245	47.086093
2565.174339	241.029897	47.091098
2561.508354	237.338151	47.096103
2558.074933	233.637234	47.101108
2554.891619	244.480550	47.106113
2551.247389	234.051535	47.111117
2547.485584	238.315451	47.116122
2543.905018	236.873918	47.121127
2540.901741	237.839399	47.126132
2537.368566	242.305162	47.131137
2534.007569	240.106706	47.136141
2530.163552	241.710622	47.141146
2526.742796	238.475334	47.146151
2523.596021	229.908450	47.151156
2519.438130	236.802013	47.156161
2516.291172	234.691384	47.161165
2512.698256	230.826982	47.166170
2509.497487	223.674883	47.171175
2506.158182	230.505967	47.176180
2502.555827	237.187077	47.181185
2498.893061	226.571724	47.186189
2495.267406	232.159466	47.191194
2491.823750	239.880428	47.196199
2488.680470	226.578776	47.201204
2484.727100	238.484623	47.206209
2481.155207	225.707213	47.211213
2478.158498	223.336186	47.216218
2475.060706	219.441994	47.221223
2471.314416	222.093886	47.226228
2467.566543	219.969598	47.231233
2464.269439	223.580039	47.236237
2460.849154	226.220755	47.241242
2457.154308	223.176993	47.246247
2453.754757	220.590080	47.251252
2449.979258	227.412680	47.256257
2446.283214	221.973403	47.261261
2443.037195	222.425270	47.266266
2439.603369	224.874051	47.271271
2436.496941	213.572143	47.276276
2432.567710	218.087951	47.281281
2429.387361	218.008007	47.286285
2425.967387	217.899339	47.291290
2422.159082	221.275483	47.296295
2418.701485	219.597066	47.301300
2415.154455	218.410189	47.306305
2411.772087	211.986533	47.311309
2408.519875	216.411127	47.316314
2404.996718	220.546746	47.321319
2401.023146	217.962271	47.326324
2397.270465	223.869621	47.331329
2394.319739	216.181008	47.336333
2390.904631	211.933719	47.341338
2387.480147	217.048645	47.346343
2383.935782	215.306824	47.351348
2380.201793	220.362731	47.356353
2376.923095	223.820802	47.361357
2373.339223	221.376463	47.366362
2369.532226	213.945453	47.371367
2366.411791	206.527214	47.376372
2362.667037	222.110080	47.381377
2359.286141	219.099820	47.386381
2356.237107	218.188753	47.391386
2352.159890	220.285184	47.396391
2348.869562	216.049887	47.401396
2345.600162	212.723642	47.406401
2341.749115	214.464630	47.411405
2338.304176	217.459973	47.416410
2334.321483	222.341475	47.421415
2331.573067	217.515679	47.426420
2328.359857	221.188332	47.431425
2324.883377	212.389099	47.436429
2320.940927	213.528701	47.441434
2317.420933	210.993938	47.446439
2314.064307	219.296996	47.451444
2310.217878	224.084977	47.456449
2306.757533	210.849244	47.461453
2303.411378	217.490945	47.466458
2300.085779	211.039253	47.471463
2296.821995	214.210346	47.476468
2292.583059	228.482607	47.481473
2289.016516	220.756014	47.486477
2285.958639	219.689961	47.491482
2282.496219	219.379219	47.496487
2278.947771	211.749308	47.501492
2275.552971	212.928381	47.506497
2272.182186	212.273354	47.511501
2268.380390	211.086022	47.516506
2265.160723	219.351894	47.521511
2261.203270	217.266514	47.526516
2257.863045	221.901298	47.531521
2254.757308	214.250412	47.536525
2251.517906	223.049411	47.541530
2247.212546	213.710212	47.546535
2244.285934	208.784438	47.551540
2240.431291	218.164754	47.556545
2236.962475	207.435129	47.561549
2233.401918	214.169498	47.566554
2229.984663	210.026879	47.571559
2226.508048	209.791143	47.576564
2222.885093	210.322755	47.581569
2219.061507	206.595540	47.586573
2216.077313	204.068494	47.591578
2212.535717	218.016288	47.596583
2209.489534	206.913198	47.601588
2205.464250	217.371760	47.606593
2201.815921	203.963703	47.611597
2198.849513	203.048173	47.616602
2195.100632	209.055084	47.621607
2191.736995	211.216164	47.626612
2187.738484	209.465014	47.631617
2184.434979	205.817720	47.636621
2181.082663	206.923338	47.641626
2177.393161	203.184478	47.646631
2174.057937	201.386180	47.651636
2170.613113	212.775681	47.656641
2167.132871	202.536224	47.661645
2163.769060	202.492864	47.666650
2159.838835	206.519438	47.671655
2156.364040	198.721770	47.676660
2152.922359	211.626138	47.681665
2149.531526	202.755089	47.686669
2146.218288	201.141641	47.691674
2142.519934	206.650447	47.696679
2138.986716	201.533044	47.701684
2135.714584	203.721282	47.706689
2132.356298	208.132775	47.711693
2128.667648	209.418883	47.716698
2124.693853	208.325979	47.721703
2121.570320	198.520615	47.726708
2117.686417	206.173195	47.731713
2114.741678	194.303739	47.736717
2111.135398	203.420919	47.741722
2107.536829	201.728514	47.746727
2103.968822	200.831871	47.751732
2100.428541	205.147534	47.756737
2097.164075	205.154713	47.761741
2093.527312	198.830740	47.766746
2089.937704	192.807033	47.771751
2086.552115	195.639014	47.776756
2082.668934	194.783778	47.781761
2079.522095	198.840103	47.786765
2076.201689	191.722301	47.791770
2072.462538	197.080413	47.796775
2069.267841	191.999126	47.801780
2065.464803	199.183322	47.806785
2062.007814	195.250260	47.811789
2058.460392	190.208089	47.816794
2055.041205	201.451332	47.821799
2052.010600	189.880275	47.826804
2048.092943	185.381159	47.831809
2044.435619	196.645972	47.836813
2040.854783	195.136189	47.841818
2037.305291	201.339985	47.846823
2033.932213	191.259370	47.851828
2030.363227	193.392111	47.856833
2027.184117	189.102179	47.861837
2023.755835	188.947806	47.866842
2020.265422	193.864276	47.871847
2016.654221	186.787838	47.876852
2013.030929	199.613534	47.881857
2009.297862	191.367267	47.886861
2006.063839	194.416011	47.891866
2002.575186	189.721758	47.896871
1999.181380	187.010896	47.901876
1995.555606	195.251232	47.906881
1991.830054	193.096800	47.911885
1988.610753	190.941842	47.916890
1984.664699	199.625224	47.921895
1981.691434	186.846900	47.926900
1977.843036	197.666935	47.931905
1974.642983	197.509634	47.936909
1971.302026	192.853370	47.941914
1967.631501	189.958135	47.946919
1964.178163	195.414165	47.951924
1960.315158	187.684922	47.956929
1956.576408	194.142233	47.961933
1953.661503	183.918525	47.966938
1950.003726	185.700120	47.971943
1946.621420	179.983496	47.976948
1942.977468	193.662783	47.981953
1939.508729	184.355438	47.986957
1936.299272	184.649256	47.991962
1932.428724	193.010971	47.996967
1929.018119	188.425446	48.001972
1925.445462	189.346414	48.006977
1921.708940	194.538830	48.011981
1918.545027	182.238034	48.016986
1914.929388	189.584970	48.021991
1912.077655	180.284079	48.026996
1908.167958	188.734763	48.032001
1904.634002	184.278564	48.037005
1901.191340	183.293487	48.042010
1897.500037	187.748688	48.047015
1894.215651	183.606485	48.052020
1890.167323	182.154699	48.057025
1886.724846	184.785451	48.062029
1883.617853	179.851239	48.067034
1879.977339	189.411522	48.072039
1876.328653	187.020902	48.077044
1872.684807	194.665380	48.082049
1869.400195	190.857918	48.087053
1866.195008	185.458626	48.092058
1862.583215	190.042409	48.097063
1859.441339	183.582030	48.102068
1855.758469	183.800374	48.107073
1851.940779	181.863944	48.112077
1848.333110	176.587591	48.117082
1844.728452	183.483220	48.122087
1841.478733	178.267923	48.127092
1837.994435	185.025468	48.132097
1834.478967	186.333709	48.137101
1830.658020	190.347022	48.142106
1827.058370	190.522830	48.147111
1823.875944	184.645208	48.152116
1820.240551	194.494776	48.157121
1816.924483	189.047923	48.162125
1813.503308	192.841484	48.167130
1810.199998	198.569238	48.172135
1806.677372	177.964944	48.177140
1803.162431	182.230050	48.182145
1799.618920	185.472729	48.187149
1796.289131	182.523910	48.192154
1792.272633	195.011335	48.197159
1789.276767	181.557259	48.202164
1785.320162	180.820369	48.207169
1781.571482	174.895229	48.212173
1778.253866	179.454152	48.217178
1774.813540	182.299924	48.222183
1771.811098	175.431174	48.227188
1767.874804	190.739942	48.232193
1764.075621	176.146157	48.237197
1760.848598	187.855114	48.242202
1757.218649	181.109181	48.247207
1754.244689	173.713777	48.252212
1750.463864	182.957504	48.257217
1746.981676	180.129412	48.262221
1743.528668	175.518083	48.267226
1739.978999	177.116013	48.272231
1736.283921	180.292211	48.277236
1732.873136	179.944922	48.282241
1729.281566	175.194086	48.287245
1725.711736	179.187106	48.292250
1722.531132	175.929133	48.297255
1719.378052	166.983258	48.302260
1715.311106	174.634193	48.307265
1711.809337	172.472226	48.312269
1708.230784	171.007319	48.317274
1704.432690	177.014809	48.322279
1701.229500	170.116722	48.327284
1697.939026	177.091377	48.332289
1694.866995	172.430760	48.337293
1691.441667	169.006433	48.342298
1687.499623	180.732721	48.347303
1684.001529	174.720480	48.352308
1680.035950	175.099140	48.357313
1676.647183	164.758573	48.362317
1673.402148	174.998202	48.367322
1669.327592	176.120886	48.372327
1666.569062	173.168162	48.377332
1662.749769	166.776050	48.382337
1659.416918	175.643301	48.387341
1656.175647	172.743309	48.392346
1652.328650	182.618077	48.397351
1648.866454	169.356811	48.402356
1645.219330	177.368833	48.407361
1641.879362	168.967173	48.412365
1638.502847	168.795448	48.417370
1634.504265	177.051046	48.422375
1631.501729	172.427339	48.427380
1627.728725	169.123656	48.432385
1624.402386	167.000260	48.437389
1621.113129	165.773762	48.442394
1616.879206	176.308052	48.447399
1613.491746	159.087705	48.452404
1610.053378	164.891765	48.457409
1606.759841	168.932358	48.462413
1603.302353	161.021594	48.467418
1599.372343	169.860268	48.472423
1596.542674	159.884621	48.477428
1593.173418	177.193164	48.482433
1589.658352	170.360115	48.487437
1586.098841	170.124733	48.492442
1582.415813	165.302107	48.497447
1578.692022	163.607129	48.502452
1575.245111	163.732632	48.507457
1571.535985	168.083858	48.512461
1568.152108	166.990646	48.517466
1564.715047	172.198166	48.522471
1561.260900	155.728910	48.527476
1557.809750	161.209113	48.532481
1554.097909	159.015678	48.537485
1551.048202	160.604145	48.542490
1547.191660	165.838171	48.547495
1543.935830	159.397655	48.552500
1540.235294	168.504721	48.557505
1536.788543	163.818523	48.562509
1533.348959	155.945316	48.567514
1529.503552	164.134235	48.572519
1526.573771	160.517440	48.577524
1522.627954	167.347510	48.582529
1518.879876	160.653278	48.587533
1515.873966	156.799637	48.592538
1512.120354	172.721299	48.597543
1508.557656	157.877349	48.602548
1505.085107	167.460040	48.607553
1501.663284	164.041004	48.612557
1498.551074	164.367199	48.617562
1494.421574	166.295374	48.622567
1491.293234	163.700475	48.627572
1488.036415	166.369300	48.632577
1484.333732	165.281476	48.637581
1480.789036	163.543364	48.642586
1476.898130	168.266098	48.647591
1473.831050	160.137195	48.652596
1470.000545	162.969516	48.657601
1466.727394	169.583084	48.662605
1463.052315	161.843573	48.667610
1459.527101	160.375572	48.672615
1456.301758	159.105083	48.677620
1453.057253	169.239569	48.682625
1449.397039	165.250591	48.687629
1445.707138	168.023779	48.692634
1441.662653	167.266779	48.697639
1438.318900	160.202683	48.702644
1435.433727	168.143185	48.707649
1431.717087	165.885521	48.712653
1428.329891	163.487570	48.717658
1424.533204	168.078147	48.722663
1421.326628	170.322725	48.727668
1417.620551	171.747039	48.732673
1414.422406	160.356727	48.737677
1410.499286	156.000379	48.742682
1406.880443	166.320689	48.747687
1403.643481	150.996953	48.752692
1400.350470	164.250715	48.757697
1396.427826	163.260492	48.762701
1393.073060	164.257737	48.767706
1389.605421	162.240950	48.772711
1386.139692	163.551166	48.777716
1382.764239	165.915247	48.782721
1379.137802	163.150557	48.787725
1375.756265	156.336668	48.792730
1372.091221	165.676764	48.797735
1369.015009	150.272024	48.802740
1365.170522	154.329049	48.807745
1361.616119	159.831781	48.812749
1357.857364	149.409577	48.817754
1354.323796	159.139597	48.822759
1351.133843	148.239166	48.827764
1347.683187	153.994913	48.832769
1343.910836	161.155603	48.837773
1340.780854	156.570339	48.842778
1336.750243	164.207867	48.847783
1333.424241	158.401913	48.852788
1330.444306	155.543820	48.857793
1326.394150	154.841536	48.862797
1323.140736	149.915364	48.867802
1319.501448	159.598748	48.872807
1316.289746	148.876386	48.877812
1312.178286	166.307360	48.882817
1309.041894	160.043832	48.887821
1305.779016	157.865783	48.892826
1302.070635	155.856890	48.897831
1298.419206	144.835844	48.902836
1295.400137	152.190551	48.907841
1291.519613	153.460868	48.912845
1287.755408	153.530697	48.917850
1284.080391	154.637003	48.922855
1281.244728	144.173976	48.927860
1277.800412	155.478253	48.932865
1274.558335	144.208010	48.937869
1270.532851	156.874876	48.942874
1266.698627	164.030461	48.947879
1263.391158	156.737913	48.952884
1260.233107	145.816102	48.957889
1256.610561	148.158759	48.962893
1253.042870	149.308326	48.967898
1248.906563	154.540482	48.972903
1245.627344	145.646822	48.977908
1242.603771	149.110018	48.982913
1239.098868	154.163604	48.987917
1235.593796	142.765977	48.992922
1231.856968	159.202845	48.997927
1228.809985	152.242799	49.002932
1225.357635	160.599625	49.007937
1221.622863	158.321060	49.012941
1217.934452	152.913349	49.017946
1214.260225	159.503789	49.022951
1211.055775	155.144846	49.027956
1207.276110	154.833870	49.032961
1203.811897	151.960612	49.037965
1200.456115	155.305495	49.042970
1196.925347	161.561031	49.047975
1193.527995	149.843503	49.052980
1190.155513	157.637366	49.057985
1186.388576	153.428465	49.062989
1182.911115	156.208174	49.067994
1179.328039	156.368917	49.072999
1175.961236	154.195911	49.078004
1172.425443	153.121206	49.083009
1169.010172	154.872974	49.088013
1165.568885	158.755160	49.093018
1161.864770	154.781974	49.098023
1158.454367	149.466488	49.103028
1154.891226	153.131825	49.108033
1151.190301	151.738111	49.113037
1147.975888	148.360053	49.118042
1144.408351	146.302156	49.123047
1140.907917	141.964184	49.128052
1137.460585	153.258391	49.133057
1133.833365	154.970437	49.138061
1130.344560	141.208087	49.143066
1126.747873	151.298570	49.148071
1123.597733	148.872909	49.153076
1119.920857	154.470459	49.158081
1116.302443	146.197767	49.163085
1113.096109	138.931845	49.168090
1109.373307	148.856706	49.173095
1105.720282	144.082025	49.178100
1102.661358	144.669438	49.183105
1098.643741	142.293297	49.188109
1095.662767	148.006684	49.193114
1091.516179	148.719283	49.198119
1088.335353	145.678096	49.203124
1084.529798	145.957399	49.208129
1081.078825	144.895975	49.213133
1078.188147	135.670624	49.218138
1074.510951	145.270057	49.223143
1070.958770	147.258448	49.228148
1067.211465	150.247637	49.233153
1063.691964	146.896606	49.238157
1060.444524	147.913642	49.243162
1056.640322	148.255892	49.248167
1053.187643	143.131995	49.253172
1049.979114	153.941184	49.258177
1046.236609	143.903371	49.263181
1043.049324	145.293702	49.268186
1039.227706	145.193062	49.273191
1035.640946	152.602129	49.278196
1032.106325	144.914970	49.283201
1028.554279	145.577660	49.288205
1025.554282	141.249779	49.293210
1022.116924	146.047060	49.298215
1018.444663	141.175981	49.303220
1014.732907	144.686815	49.308225
1011.008885	152.923338	49.313229
1007.571599	144.546199	49.318234
1003.789091	160.654509	49.323239
1000.992570	147.643708	49.328244
997.245066	147.076380	49.333249
993.905542	149.540570	49.338253
990.401675	149.374796	49.343258
986.715449	157.667053	49.348263
983.571719	153.405000	49.353268
979.863642	156.468286	49.358273
976.195434	166.387383	49.363277
972.952998	146.034219	49.368282
969.167601	152.866412	49.373287
965.881678	156.115448	49.378292
962.108896	150.327635	49.383297
958.300652	153.418356	49.388301
955.336669	151.746446	49.393306
951.650736	156.529436	49.398311
948.179836	155.225331	49.403316
944.909621	143.861350	49.408321
941.075006	152.943254	49.413325
937.829783	141.010765	49.418330
934.151450	140.454153	49.423335
930.659980	141.291215	49.428340
927.427824	140.524262	49.433345
923.576499	149.647422	49.438349
920.274107	140.519877	49.443354
916.493915	152.579491	49.448359
913.136058	144.032216	49.453364
909.706236	146.190728	49.458369
906.136296	146.073047	49.463373
902.990910	142.007287	49.468378
899.000140	148.550854	49.473383
895.765411	134.099836	49.478388
892.632772	142.149240	49.483393
888.721202	137.100786	49.488397
885.183954	140.433870	49.493402
881.340667	145.361536	49.498407
877.968451	141.449346	49.503412
874.511133	146.495718	49.508417
870.955641	155.750555	49.513421
868.346133	141.440646	49.518426
864.165245	143.626128	49.523431
860.777130	147.127561	49.528436
857.174583	146.554926	49.533441
853.677740	151.591078	49.538445
849.974732	142.615300	49.543450
846.541539	150.788252	49.548455
842.955039	140.146831	49.553460
839.610070	148.557588	49.558465
835.863991	144.299965	49.563469
832.670755	138.888050	49.568474
829.010548	140.848516	49.573479
825.687630	145.460062	49.578484
822.449453	148.880481	49.583489
818.672497	148.151230	49.588493
815.440560	133.325277	49.593498
811.407387	150.643796	49.598503
807.725316	138.100894	49.603508
804.314837	145.526946	49.608513
800.864726	142.174522	49.613517
797.794000	140.819934	49.618522
794.351908	145.731038	49.623527
790.620043	141.464199	49.628532
786.735752	138.972755	49.633537
783.567062	142.818411	49.638541
780.218351	136.151345	49.643546
776.322650	146.644367	49.648551
773.176992	136.256091	49.653556
769.681423	141.581189	49.658561
765.736110	140.001094	49.663565
763.016679	137.558916	49.668570
759.189966	136.674553	49.673575
755.400079	140.603056	49.678580
751.971677	142.881234	49.683585
748.596104	136.283166	49.688589
744.781237	136.538644	49.693594
741.547278	141.772731	49.698599
738.190947	144.345657	49.703604
734.578372	143.702557	49.708609
730.513760	144.105134	49.713613
727.395834	138.025094	49.718618
724.069064	137.764324	49.723623
720.675836	136.922344	49.728628
716.892921	133.638268	49.733633
713.682498	142.008495	49.738637
710.025694	137.616238	49.743642
706.610809	135.039319	49.748647
703.120854	132.915278	49.753652
699.639445	134.951251	49.758657
695.745456	138.355139	49.763661
692.296766	136.744458	49.768666
688.748733	143.831825	49.773671
685.644681	137.268417	49.778676
681.779407	148.473797	49.783681
678.252455	150.724921	49.788685
675.135666	140.974671	49.793690
671.404657	146.654729	49.798695
668.056286	141.458248	49.803700
664.775587	148.954294	49.808705
661.151105	143.325549	49.813709
657.644078	136.223405	49.818714
654.030860	145.981280	49.823719
650.362897	133.782526	49.828724
647.291383	144.854632	49.833729
643.378843	148.482258	49.838733
639.842241	134.789454	49.843738
635.991182	140.906175	49.848743
632.699275	142.894469	49.853748
629.471661	140.064032	49.858753
625.903071	135.992529	49.863757
622.752625	131.372913	49.868762
618.759251	129.749598	49.873767
615.466140	143.996423	49.878772
612.224734	143.151905	49.883777
608.321453	148.212267	49.888781
605.163077	138.780156	49.893786
601.251907	142.570589	49.898791
597.644761	144.583835	49.903796
594.516400	141.420279	49.908801
590.644717	151.299113	49.913805
587.855212	148.427989	49.918810
583.583310	148.681674	49.923815
580.465541	138.187905	49.928820
576.782816	141.903856	49.933825
573.004815	143.616038	49.938829
569.943989	136.558740	49.943834
566.293773	147.446038	49.948839
562.972836	135.809384	49.953844
559.509125	143.006821	49.958849
555.802207	135.179085	49.963853
552.492669	140.867839	49.968858
548.886033	143.807335	49.973863
545.490005	143.101130	49.978868
541.842084	135.106368	49.983873
538.203516	135.331275	49.988877
534.785743	132.799769	49.993882
531.301576	133.392817	49.998887
528.028936	128.908147	50.003892
524.533841	133.767633	50.008897
520.597213	142.361359	50.013901
517.424140	137.599932	50.018906
513.597353	142.782891	50.023911
510.359426	142.441869	50.028916
507.228398	139.784987	50.033921
503.159488	144.510141	50.038925
499.621939	144.772039	50.043930
496.059663	152.973305	50.048935
492.478916	136.731260	50.053940
489.287294	138.275043	50.058945
485.825906	150.594596	50.063949
482.442847	134.839632	50.068954
478.519406	136.597669	50.073959
475.165880	144.545950	50.078964
471.965323	139.290636	50.083969
467.823420	141.994356	50.088973
464.827049	139.244970	50.093978
461.608030	151.041747	50.098983
458.242033	140.587578	50.103988
454.430901	135.566327	50.108993
450.552909	143.736200	50.113997
447.237838	146.289687	50.119002
443.782658	144.876036	50.124007
440.579290	141.401181	50.129012
436.808900	136.735315	50.134017
432.809762	145.710056	50.139021
429.555127	148.963766	50.144026
426.139388	145.012770	50.149031
422.816824	133.051698	50.154036
418.807288	139.219886	50.159041
415.568135	139.751362	50.164045
412.376116	129.163466	50.169050
409.007438	141.845026	50.174055
405.419493	137.017766	50.179060
401.634459	140.499779	50.184065
398.284078	142.906211	50.189069
394.588865	142.291674	50.194074
391.104953	140.067826	50.199079
387.701249	136.650245	50.204084
384.257844	139.058269	50.209089
380.513552	151.150616	50.214093
377.346154	138.664442	50.219098
373.649561	149.307559	50.224103
370.243659	145.423260	50.229108
366.738076	139.646241	50.234113
362.643038	141.446990	50.239117
359.765100	139.701855	50.244122
356.055890	142.343338	50.249127
352.684889	147.410341	50.254132
349.300552	143.331667	50.259137
345.762079	143.703956	50.264141
342.369977	136.234574	50.269146
338.710691	144.785901	50.274151
334.770975	140.161178	50.279156
331.519715	135.033956	50.284161
327.979616	147.388347	50.289165
325.187146	138.810948	50.294170
321.222354	152.007619	50.299175
317.702994	139.021097	50.304180
314.144289	134.231901	50.309185
310.564515	148.196419	50.314189
307.273180	143.680877	50.319194
303.606808	151.621864	50.324199
300.067257	147.696006	50.329204
296.800875	154.320275	50.334209
292.793880	146.215861	50.339213
289.489893	137.868004	50.344218
285.617423	142.028031	50.349223
282.318160	135.853838	50.354228
279.171890	137.149911	50.359233
275.754385	140.255062	50.364237
272.011538	144.463304	50.369242
268.532993	144.443892	50.374247
264.968589	142.642352	50.379252
261.944755	141.600268	50.384257
257.998818	145.241254	50.389261
254.596692	139.123973	50.394266
251.379446	141.716862	50.399271
247.704355	140.050088	50.404276
244.008006	138.560491	50.409281
239.864356	144.725777	50.414285
236.607570	131.355273	50.419290
233.154264	134.973336	50.424295
230.414830	141.955604	50.429300
226.912726	129.814468	50.434305
222.961395	134.698797	50.439309
219.953683	132.908346	50.444314
215.913488	134.341398	50.449319
212.378608	137.769925	50.454324
209.200141	143.423805	50.459329
205.370952	142.174091	50.464333
201.881111	131.424726	50.469338
198.275195	140.419812	50.474343
194.928347	142.223940	50.479348
191.879931	137.453578	50.484353
188.010520	139.053745	50.489357
184.408947	126.082157	50.494362
180.721642	142.551181	50.499367
177.447786	136.933302	50.504372
173.758506	139.195122	50.509377
170.000294	136.497090	50.514381
167.185724	128.714394	50.519386
163.570382	138.395620	50.524391
159.997825	140.122293	50.529396
156.702822	130.381066	50.534401
152.907514	137.298817	50.539405
149.544081	128.493836	50.544410
145.964223	135.015984	50.549415
141.937365	138.564105	50.554420
138.713311	136.951217	50.559425
135.174120	143.263979	50.564429
132.093016	132.100487	50.569434
128.904953	137.621032	50.574439
125.109836	140.714226	50.579444
121.573688	134.534792	50.584449
117.204732	136.223650	50.589453
114.285717	130.264098	50.594458
111.059897	134.999987	50.599463
107.852689	137.200201	50.604468
104.204397	132.708608	50.609473
100.501936	134.015400	50.614477
97.239253	128.517300	50.619482
93.302309	133.423830	50.624487
89.664365	131.625540	50.629492
86.504004	130.578366	50.634497
82.814820	132.489188	50.639501
79.307965	131.842950	50.644506
75.673523	132.864008	50.649511
72.491903	132.464465	50.654516
69.240612	119.471505	50.659521
65.238473	130.188522	50.664525
61.760831	129.291582	50.669530
58.085938	134.013659	50.674535
54.806514	134.668108	50.679540
51.741424	127.661855	50.684545
48.153322	127.109807	50.689549
44.255680	128.196772	50.694554
40.580751	139.299690	50.699559
37.214128	135.193680	50.704564
33.955996	127.206290	50.709569
30.098080	130.580707	50.714573
26.710745	119.195109	50.719578
23.426418	132.991699	50.724583
19.782769	131.252432	50.729588
16.736945	132.438921	50.734593
13.019641	133.574394	50.739597
9.694953	124.267420	50.744602
5.697254	137.096814	50.749607
2.295820	126.092846	50.754612